Tue Jun 21 10:37:18 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.636588	101.926405	0.000000
0.640675	97.647972	0.005005
0.886987	98.874142	0.010010
0.507638	98.407187	0.015014
0.587971	87.799443	0.020019
0.367297	79.376910	0.025024
0.556714	74.076976	0.030029
0.279703	60.523614	0.035034
-0.144632	51.480264	0.040038
-0.237580	39.304814	0.045043
-0.832087	32.620171	0.050048
-0.817917	17.382137	0.055053
-1.465816	15.656266	0.060058
-1.749597	10.447147	0.065062
-1.560892	5.743302	0.070067
-2.543588	-4.298214	0.075072
-2.527368	-10.813626	0.080077
-3.163439	-9.026153	0.085082
-3.277374	-8.744368	0.090086
-3.221701	2.022078	0.095091
-3.765711	-4.098840	0.100096
-4.065721	-7.095327	0.105101
-4.599421	-7.731289	0.110106
-4.775155	-4.299496	0.115110
-4.625779	-5.853103	0.120115
-5.158554	3.784165	0.125120
-5.124086	-1.282686	0.130125
-5.414546	-0.360329	0.135130
-5.978769	-3.822775	0.140134
-6.283028	-10.286694	0.145139
-6.587248	4.293423	0.150144
-6.560332	-12.511547	0.155149
-6.629424	-8.549026	0.160154
-6.613799	-8.246466	0.165158
-6.682219	-4.661949	0.170163
-7.563639	0.711647	0.175168
-7.500439	1.511108	0.180173
-7.394977	3.181704	0.185178
-8.363057	-3.055270	0.190182
-8.634548	-7.364801	0.195187
-9.319947	-6.100775	0.200192
-9.429173	-11.029373	0.205197
-9.394541	-9.791444	0.210202
-9.315249	-4.919909	0.215206
-9.292707	-5.825781	0.220211
-9.950527	6.091863	0.225216
-10.452837	-2.749890	0.230221
-10.988253	-3.632826	0.235226
-10.985038	-11.385535	0.240230
-10.931590	-11.160871	0.245235
-11.028749	3.358514	0.250240
-11.128398	-3.928428	0.255245
-11.915663	0.781138	0.260250
-12.573888	-2.340535	0.265254
-12.326670	-9.550926	0.270259
-12.680280	-2.610687	0.275264
-12.570123	-3.900675	0.280269
-12.434981	-1.802833	0.285274
-13.159404	2.339254	0.290278
-13.667704	-0.927620	0.295283
-13.961764	7.229584	0.300288
-13.787110	-0.663606	0.305293
-13.928372	2.348474	0.310298
-15.040702	0.832718	0.315302
-15.334439	-4.922939	0.320307
-15.792218	4.474386	0.325312
-15.920189	-7.215310	0.330317
-15.272586	-3.055147	0.335322
-15.475662	-1.662018	0.340326
-15.383443	-9.027104	0.345331
-15.605468	2.213542	0.350336
-16.295307	-7.977499	0.355341
-17.051399	-5.062911	0.360346
-17.020720	-8.709514	0.365350
-17.192188	-10.761930	0.370355
-17.896569	1.410087	0.375360
-18.671177	-2.779619	0.380365
-18.037176	-1.685938	0.385370
-18.482274	3.214620	0.390374
-18.183437	-6.765609	0.395379
-18.942339	1.377797	0.400384
-18.705619	-14.239037	0.405389
-18.974497	-13.530217	0.410394
-19.451957	-19.059096	0.415398
-19.923089	-8.914832	0.420403
-20.479376	-2.108960	0.425408
-20.130056	-6.098412	0.430413
-20.319733	0.898745	0.435418
-20.778895	-8.049011	0.440422
-21.520996	-11.597634	0.445427
-21.809066	-0.984625	0.450432
-22.132255	-8.456150	0.455437
-22.110892	-6.939559	0.460442
-22.168594	-0.082658	0.465446
-21.883910	-7.492838	0.470451
-22.680043	0.498275	0.475456
-22.446462	-2.377796	0.480461
-22.764908	-0.729155	0.485466
-23.314885	6.443111	0.490470
-23.633536	-1.506124	0.495475
-23.956771	-3.787179	0.500480
-24.173918	-2.798817	0.505485
-23.885744	4.320290	0.510490
-24.514306	-4.669271	0.515494
-24.970169	-0.376099	0.520499
-25.602579	0.626962	0.525504
-25.238718	-7.187643	0.530509
-25.451741	-3.813414	0.535514
-25.586125	-1.936944	0.540518
-25.839365	-6.363357	0.545523
-26.757231	2.272083	0.550528
-26.619619	-6.741744	0.555533
-26.881236	0.567668	0.560538
-27.276635	0.856007	0.565542
-27.183887	-0.926011	0.570547
-27.126312	-1.525700	0.575552
-27.331897	-8.778124	0.580557
-28.070583	-6.586487	0.585562
-28.677755	-3.204803	0.590566
-28.605227	4.868603	0.595571
-28.561595	2.374452	0.600576
-29.052685	2.833347	0.605581
-29.760790	-3.894818	0.610586
-30.014609	5.673760	0.615590
-30.019643	-5.885334	0.620595
-30.410154	0.755348	0.625600
-30.281857	-0.223883	0.630605
-30.239832	-6.997339	0.635610
-30.379582	0.776937	0.640614
-30.814973	-7.701549	0.645619
-31.396072	6.382544	0.650624
-31.318982	-1.729512	0.655629
-31.583825	-2.308960	0.660634
-32.481558	-2.073197	0.665638
-32.651936	-1.278864	0.670643
-33.250389	-7.245126	0.675648
-33.063165	-0.965140	0.680653
-32.922741	-10.092108	0.685658
-33.228051	0.775949	0.690662
-32.981721	2.857745	0.695667
-33.594239	1.579100	0.700672
-34.153591	-3.846236	0.705677
-34.290870	-1.089771	0.710682
-34.593861	4.029382	0.715686
-34.655766	-6.396082	0.720691
-35.024203	3.896943	0.725696
-35.580992	8.662080	0.730701
-35.927780	2.461736	0.735706
-36.331134	8.441705	0.740710
-36.089586	1.777481	0.745715
-36.698263	3.966535	0.750720
-36.339979	-2.785888	0.755725
-36.055010	0.206319	0.760730
-36.839700	2.788208	0.765734
-37.333255	-4.811194	0.770739
-37.622234	12.973074	0.775744
-38.143340	5.243846	0.780749
-37.906040	7.250177	0.785754
-38.485849	2.154026	0.790758
-39.267594	7.003185	0.795763
-39.196384	6.836160	0.800768
-39.197758	-4.513774	0.805773
-39.570732	-2.034602	0.810778
-39.591286	2.889778	0.815782
-39.629022	-11.226863	0.820787
-39.685589	2.869619	0.825792
-39.835111	-6.507109	0.830797
-40.666867	-1.316966	0.835802
-40.859134	0.688082	0.840806
-40.886169	0.408074	0.845811
-41.289224	0.518305	0.850816
-42.118564	3.016224	0.855821
-42.600996	-4.468395	0.860826
-42.160829	8.546335	0.865830
-42.135649	-0.199643	0.870835
-42.733056	7.324234	0.875840
-42.676382	0.408835	0.880845
-42.530968	-2.224321	0.885850
-43.675212	-4.968315	0.890854
-43.825443	-6.232545	0.895859
-44.186756	-3.186589	0.900864
-44.295906	0.116764	0.905869
-44.132564	-0.912277	0.910874
-44.088564	-5.567684	0.915878
-44.630423	-4.198566	0.920883
-45.554676	-0.757067	0.925888
-45.750136	-0.939326	0.930893
-45.620640	-5.990338	0.935898
-45.645070	2.571736	0.940902
-45.589888	-2.405007	0.945907
-46.476951	0.957123	0.950912
-47.021716	1.306312	0.955917
-47.366993	-7.149207	0.960922
-47.840948	1.953809	0.965926
-47.525513	-4.483678	0.970931
-47.798552	2.918991	0.975936
-47.672302	2.783699	0.980941
-47.882210	1.162311	0.985946
-47.920110	3.280718	0.990950
-47.763222	-8.432862	0.995955
-48.628873	1.822329	1.000960
-48.959822	-2.123928	1.005965
-49.532173	-9.192867	1.010970
-50.744244	-2.437243	1.015974
-49.982968	-3.851441	1.020979
-50.062008	-5.248032	1.025984
-50.216542	-10.211353	1.030989
-50.791433	-10.549420	1.035994
-50.823523	-10.838655	1.040998
-50.875844	-7.007376	1.046003
-51.252836	-2.238667	1.051008
-51.952044	-7.602160	1.056013
-52.079016	-3.498628	1.061018
-52.424439	-8.839804	1.066022
-52.432546	-13.501576	1.071027
-52.509653	1.034016	1.076032
-52.315791	-5.013928	1.081037
-53.026925	-11.479130	1.086042
-53.845533	-8.212402	1.091046
-53.816771	-8.322077	1.096051
-54.137805	-4.581469	1.101056
-54.187263	-2.529426	1.106061
-53.983464	-3.497482	1.111066
-54.376720	3.228510	1.116070
-54.929204	-7.702576	1.121075
-55.151217	-2.477646	1.126080
-55.273499	-7.396186	1.131085
-55.172855	-4.861855	1.136090
-56.192016	-2.653166	1.141094
-56.866651	-3.981903	1.146099
-56.436964	-4.232568	1.151104
-56.855585	-0.619259	1.156109
-57.158995	-3.115925	1.161114
-57.401428	-3.385322	1.166118
-57.292068	-3.511502	1.171123
-57.353898	-5.726719	1.176128
-57.612743	-8.619314	1.181133
-57.985168	-6.273235	1.186138
-58.346892	-10.868749	1.191142
-58.399391	-7.083617	1.196147
-58.674604	2.680507	1.201152
-58.803044	-1.533521	1.206157
-59.491078	-8.116804	1.211162
-60.057074	-8.459895	1.216166
-60.061410	-7.007918	1.221171
-60.312054	-5.059309	1.226176
-60.477661	-3.779930	1.231181
-60.131654	-1.915530	1.236186
-60.948277	-1.603407	1.241190
-61.273754	-0.059567	1.246195
-61.897875	2.651824	1.251200
-62.226980	-2.770001	1.256205
-61.882604	-0.037064	1.261210
-61.994634	1.574434	1.266214
-61.914392	-9.415654	1.271219
-62.446068	1.541198	1.276224
-63.415210	-3.887898	1.281229
-63.504130	-5.326266	1.286234
-63.819077	-2.790004	1.291238
-63.721185	-8.559599	1.296243
-63.596948	0.409616	1.301248
-63.478405	-9.800639	1.306253
-64.225109	-2.892978	1.311258
-64.836677	2.551376	1.316262
-64.948619	-0.443298	1.321267
-64.764051	-1.380345	1.326272
-65.388524	0.606101	1.331277
-66.071141	-16.060824	1.336282
-66.251955	-1.641459	1.341286
-66.281470	-9.343555	1.346291
-66.319538	-11.439175	1.351296
-66.699639	-0.629972	1.356301
-66.533508	-0.482381	1.361306
-66.741722	-6.553127	1.366310
-67.341708	-9.374818	1.371315
-67.787605	4.603015	1.376320
-68.192733	-2.916503	1.381325
-68.150324	-7.408056	1.386330
-68.317248	-2.203498	1.391334
-68.735242	2.101363	1.396339
-69.413117	-8.625037	1.401344
-69.765572	0.577834	1.406349
-69.439768	-7.886799	1.411354
-70.151450	-3.822592	1.416358
-69.873646	-7.639966	1.421363
-70.178005	-13.457000	1.426368
-70.211229	-9.146799	1.431373
-69.951363	-9.117741	1.436378
-70.741271	-5.744072	1.441382
-71.031777	-12.411736	1.446387
-71.519360	-5.254542	1.451392
-71.656562	-6.085217	1.456397
-71.849554	-7.404129	1.461402
-72.935032	-7.797344	1.466406
-73.065996	-10.087740	1.471411
-73.088572	-5.609793	1.476416
-72.678299	-8.788039	1.481421
-73.068711	-4.068612	1.486426
-73.500472	-5.733965	1.491430
-73.430302	-14.254924	1.496435
-73.736404	-5.275616	1.501440
-74.213816	-1.691049	1.506445
-74.582183	-14.706858	1.511450
-74.916522	-0.974243	1.516454
-74.835743	-15.981728	1.521459
-75.020993	2.616512	1.526464
-75.248664	2.390650	1.531469
-76.186036	-6.957812	1.536474
-76.582893	6.580135	1.541478
-76.420138	3.838335	1.546483
-76.677950	-6.009249	1.551488
-76.612537	-0.292608	1.556493
-76.600256	-1.645517	1.561498
-76.589588	-2.792143	1.566502
-77.174028	-10.257885	1.571507
-78.176254	-8.898161	1.576512
-78.155589	0.377299	1.581517
-77.795660	-8.679855	1.586522
-78.432500	-0.026622	1.591526
-78.242746	-6.287202	1.596531
-79.315066	-8.016765	1.601536
-79.780321	-6.848783	1.606541
-79.816939	-4.425316	1.611546
-79.843850	0.229965	1.616550
-80.184480	-1.737798	1.621555
-80.328010	-5.435074	1.626560
-80.348772	1.728283	1.631565
-80.084175	-4.794912	1.636570
-80.494186	-5.190474	1.641574
-80.906702	-4.984347	1.646579
-81.009506	-5.188264	1.651584
-81.696998	-8.620217	1.656589
-82.856572	-12.024502	1.661594
-82.829962	-13.675388	1.666598
-82.337841	-13.384258	1.671603
-82.812333	-5.558890	1.676608
-82.955551	-5.570424	1.681613
-82.975833	-6.802894	1.686618
-83.496023	3.788964	1.691622
-83.373390	-17.751859	1.696627
-84.057241	5.912415	1.701632
-84.325595	6.305419	1.706637
-84.363817	0.614802	1.711642
-84.555091	1.828577	1.716646
-84.790476	-6.824511	1.721651
-85.258294	1.127034	1.726656
-85.941959	-2.964055	1.731661
-86.108200	-14.428356	1.736666
-86.314076	-4.509764	1.741670
-86.221921	-4.481938	1.746675
-86.453267	-12.538956	1.751680
-86.442654	-5.932544	1.756685
-86.421998	-12.625692	1.761690
-87.128685	-3.879393	1.766694
-87.405329	-1.785186	1.771699
-87.529759	-7.247021	1.776704
-87.817248	1.053933	1.781709
-88.097198	-9.418685	1.786714
-88.910494	2.034729	1.791718
-89.255968	3.917350	1.796723
-89.329335	0.666267	1.801728
-89.592315	-10.588233	1.806733
-89.399989	-0.309941	1.811738
-89.938387	7.539831	1.816742
-89.560006	-5.862704	1.821747
-89.610759	3.600409	1.826752
-90.322374	8.648910	1.831757
-90.553214	-5.599729	1.836762
-91.396199	-0.597356	1.841766
-91.174239	-2.624352	1.846771
-91.253713	9.130220	1.851776
-91.753652	8.250891	1.856781
-92.286071	-2.855587	1.861786
-92.923402	8.220987	1.866790
-92.599866	-7.099819	1.871795
-92.694909	1.400142	1.876800
-93.164483	-6.171843	1.881805
-92.948730	-1.993848	1.886810
-93.114232	5.885727	1.891814
-93.739432	6.574633	1.896819
-94.164505	1.248033	1.901824
-94.473982	-2.817806	1.906829
-94.255022	-4.142193	1.911834
-94.598185	0.328665	1.916838
-94.956701	-6.132572	1.921843
-95.520064	2.817716	1.926848
-96.237589	-1.676046	1.931853
-95.569258	-10.854922	1.936858
-95.774274	0.015268	1.941862
-95.789757	-2.096131	1.946867
-96.243754	-1.937990	1.951872
-96.935555	2.530225	1.956877
-96.802074	-7.656257	1.961882
-97.494641	-4.898993	1.966886
-97.474808	-3.635723	1.971891
-97.350635	-1.319398	1.976896
-98.423268	-0.474296	1.981901
-98.746693	-1.929669	1.986906
-99.049920	-2.031918	1.991910
-98.772366	-0.428702	1.996915
-99.121991	4.538298	2.006912
-98.194330	1.423178	2.016909
-98.064119	0.587301	2.026906
-98.001514	-3.726748	2.036902
-97.307658	1.202648	2.046899
-96.539694	5.204552	2.056896
-96.324385	-0.414357	2.066893
-96.019721	-1.908833	2.076890
-95.087938	-2.284511	2.086886
-95.220707	1.441566	2.096883
-94.233648	5.318271	2.106880
-93.518788	0.846007	2.116877
-93.351488	-0.182929	2.126874
-92.480916	3.892872	2.136870
-91.821505	-2.310546	2.146867
-91.620017	7.899877	2.156864
-91.655678	3.682122	2.166861
-90.496110	-1.316858	2.176858
-90.532260	2.565709	2.186854
-89.802940	5.008738	2.196851
-88.845070	2.917843	2.206848
-88.845263	1.919413	2.216845
-88.371364	3.863162	2.226842
-87.419798	2.376344	2.236838
-87.202883	-1.178846	2.246835
-87.085491	-1.139862	2.256832
-85.758430	-3.231637	2.266829
-85.615452	5.722542	2.276826
-85.610671	1.986918	2.286822
-84.825000	-0.278575	2.296819
-84.414230	3.251576	2.306816
-83.128236	-5.387327	2.316813
-83.046599	-5.248765	2.326810
-82.794083	3.822420	2.336806
-82.645099	0.800700	2.346803
-81.877649	6.002437	2.356800
-81.326426	1.858989	2.366797
-80.260185	0.607672	2.376794
-79.762967	-2.664565	2.386790
-79.820135	-4.700567	2.396787
-79.752353	-2.448503	2.406784
-78.891680	-4.709622	2.416781
-78.176523	2.307700	2.426778
-77.186107	7.005812	2.436774
-76.834173	0.505566	2.446771
-76.726983	3.212665	2.456768
-76.572869	-3.094378	2.466765
-75.579032	0.915567	2.476762
-75.256408	3.946989	2.486758
-74.745645	-3.504659	2.496755
-73.965688	0.402398	2.506752
-73.276296	-2.154789	2.516749
-73.116486	-3.966901	2.526746
-73.023414	-4.506767	2.536742
-72.222457	-3.602940	2.546739
-71.896718	-4.961804	2.556736
-70.914735	-5.991700	2.566733
-70.464781	-0.334898	2.576730
-70.397557	2.768065	2.586726
-69.942172	0.836661	2.596723
-69.086361	-3.902171	2.606720
-68.994845	-0.481561	2.616717
-67.421374	-3.509995	2.626714
-67.129318	-1.825593	2.636710
-67.253627	-1.029144	2.646707
-67.458366	-0.941551	2.656704
-66.398640	-4.512040	2.666701
-65.792480	-1.887775	2.676698
-64.721498	-3.293793	2.686694
-64.294625	0.234088	2.696691
-64.460462	8.902136	2.706688
-63.522575	6.901295	2.716685
-62.945526	9.163861	2.726682
-62.776983	8.215533	2.736678
-62.266238	8.529420	2.746675
-61.191691	8.475486	2.756672
-61.045128	9.149820	2.766669
-60.892777	4.894999	2.776666
-60.221934	-6.283947	2.786662
-59.779356	1.950996	2.796659
-59.299338	6.267338	2.806656
-58.575188	1.383153	2.816653
-58.084824	0.590376	2.826650
-57.888791	6.966956	2.836646
-56.730126	-1.756368	2.846643
-56.649884	-0.766373	2.856640
-56.543781	2.326002	2.866637
-55.418354	9.091039	2.876634
-55.002805	3.887487	2.886630
-55.103296	9.550295	2.896627
-54.026763	4.955502	2.906624
-53.435967	2.440727	2.916621
-52.951385	-3.651735	2.926618
-52.206005	-0.973268	2.936614
-52.162290	-4.487918	2.946611
-52.106797	-1.843388	2.956608
-51.154008	1.205783	2.966605
-50.437913	-3.903104	2.976602
-50.263658	-4.205283	2.986598
-49.447942	2.024805	2.996595
-48.729793	0.215662	3.006592
-48.635488	-2.173222	3.016589
-48.472613	0.367773	3.026586
-47.546079	-4.781299	3.036582
-47.146636	0.363034	3.046579
-46.728913	5.020257	3.056576
-45.765028	0.585397	3.066573
-45.605767	-1.956704	3.076570
-45.345310	-5.790785	3.086566
-44.389722	-4.363666	3.096563
-44.054452	-0.719250	3.106560
-43.793267	-2.931269	3.116557
-42.725995	-2.667855	3.126554
-42.344492	2.309922	3.136550
-42.336639	3.203233	3.146547
-41.573785	0.281390	3.156544
-40.663491	2.189230	3.166541
-40.647228	0.582078	3.176538
-40.399886	-2.893781	3.186534
-39.569903	-4.605064	3.196531
-39.164427	-6.651098	3.206528
-38.698560	-8.493345	3.216525
-37.882698	-5.281210	3.226522
-37.505731	-3.498045	3.236518
-37.320322	-2.593238	3.246515
-36.294226	4.102500	3.256512
-35.790709	0.442547	3.266509
-35.837693	-5.043022	3.276506
-35.237892	-2.540795	3.286502
-34.455927	-9.083602	3.296499
-34.236085	-11.850510	3.306496
-33.461159	-6.761443	3.316493
-32.802548	-7.405833	3.326490
-32.708787	-3.675976	3.336486
-32.064300	-3.722502	3.346483
-31.414055	-2.088325	3.356480
-31.189741	1.179097	3.366477
-30.714055	-4.463765	3.376474
-29.793802	0.528922	3.386470
-29.511561	3.738344	3.396467
-29.508164	-0.619449	3.406464
-28.326568	1.017821	3.416461
-28.102098	-3.147579	3.426458
-27.778096	-0.947626	3.436454
-26.745399	-6.085230	3.446451
-26.429697	3.732848	3.456448
-26.288417	-0.348239	3.466445
-25.612527	3.119640	3.476442
-25.198486	-1.291339	3.486438
-24.154492	-0.314533	3.496435
-23.712709	2.066466	3.506432
-23.334257	-1.552818	3.516429
-23.280860	-2.920915	3.526426
-22.887829	0.182036	3.536422
-21.841984	-3.864105	3.546419
-21.610583	0.367551	3.556416
-21.160750	3.364081	3.566413
-20.505367	-1.601379	3.576410
-20.297999	2.553248	3.586406
-19.449819	2.229961	3.596403
-18.704732	-1.628657	3.606400
-18.673565	2.356772	3.616397
-17.958067	2.519588	3.626394
-17.170428	-1.936661	3.636390
-16.937028	2.157145	3.646387
-16.918596	8.631900	3.656384
-16.188410	-1.603718	3.666381
-15.450676	-0.701067	3.676378
-14.967102	-0.302851	3.686374
-13.981215	-5.308616	3.696371
-13.643935	-5.577922	3.706368
-13.626228	1.515000	3.716365
-13.524657	5.753932	3.726362
-12.472809	0.382179	3.736358
-12.136857	-2.673071	3.746355
-11.597835	6.569015	3.756352
-10.581617	6.698037	3.766349
-10.325814	8.075275	3.776346
-10.262297	7.227129	3.786342
-9.719944	2.786801	3.796339
-9.220462	3.118366	3.806336
-8.535038	-1.034060	3.816333
-7.704147	1.554976	3.826330
-7.918606	6.176607	3.836326
-6.702595	4.720702	3.846323
-6.150075	-0.381050	3.856320
-6.163184	3.622185	3.866317
-5.729493	-2.475482	3.876314
-4.477007	-0.266076	3.886310
-4.163049	4.894793	3.896307
-4.246661	-0.974749	3.906304
-4.023372	-0.103481	3.916301
-3.033919	5.751285	3.926298
-2.986148	18.520241	3.936294
-2.427891	29.556997	3.946291
-1.953058	44.695844	3.956288
-1.555645	60.284195	3.966285
-0.987354	83.339146	3.976282
-0.394636	94.197748	3.986278
0.008195	113.587827	3.996275
0.000000	128.343543	4.001280
0.190876	146.732668	4.006285
1.050932	144.200976	4.011290
0.919816	157.241969	4.016294
1.039373	160.426576	4.021299
0.913372	175.629734	4.026304
1.045028	163.841264	4.031309
1.144364	165.369825	4.036314
0.800320	176.958973	4.041318
1.026643	180.492160	4.046323
1.016269	189.331046	4.051328
0.879448	194.548447	4.056333
1.170695	198.196392	4.061338
1.128409	202.468293	4.066342
1.277036	204.135316	4.071347
1.430144	203.010079	4.076352
1.463642	209.166820	4.081357
1.657984	201.523843	4.086362
1.385517	205.704607	4.091366
1.476709	205.983212	4.096371
1.060643	208.228207	4.101376
1.464799	205.314380	4.106381
1.301401	195.641448	4.111386
1.331440	203.841386	4.116390
1.778179	202.597667	4.121395
1.538909	203.164444	4.126400
1.315011	208.576240	4.131405
1.522024	210.351997	4.136410
1.399568	206.594540	4.141414
1.551323	199.045839	4.146419
1.408671	204.463913	4.151424
1.625517	206.209625	4.156429
1.666367	206.662723	4.161434
1.504795	207.013180	4.166438
1.424488	206.221811	4.171443
1.683441	218.671571	4.176448
1.905413	216.647310	4.181453
1.707001	210.624379	4.186458
1.441114	206.273405	4.191462
1.660117	202.513474	4.196467
1.468987	211.196020	4.201472
1.760031	225.864452	4.206477
1.938992	229.534945	4.211482
1.662776	221.488776	4.216486
1.654994	212.812070	4.221491
1.441952	223.839253	4.226496
2.021648	237.458413	4.231501
1.519800	240.015399	4.236506
1.672723	235.814107	4.241510
2.020749	232.093188	4.246515
1.517277	232.792518	4.251520
1.623742	242.226001	4.256525
1.803945	232.504238	4.261530
1.938301	248.280437	4.266534
1.847793	238.323874	4.271539
1.814467	236.693541	4.276544
1.870082	224.207995	4.281549
1.766099	236.746288	4.286554
1.810735	241.375390	4.291558
1.744752	231.190792	4.296563
2.065219	239.168603	4.301568
1.869408	232.241826	4.306573
2.372704	234.519880	4.311578
1.908955	239.142987	4.316582
2.048699	234.285365	4.321587
1.996564	241.009236	4.326592
2.069281	241.782664	4.331597
2.067267	233.477957	4.336602
1.927664	234.754626	4.341606
2.293248	240.725356	4.346611
1.818759	243.874163	4.351616
1.977221	244.869801	4.356621
1.985169	233.302851	4.361626
1.966781	247.089734	4.366630
1.813690	230.433301	4.371635
2.273493	235.616840	4.376640
1.910483	236.450978	4.381645
1.981276	230.865552	4.386650
1.812660	246.204894	4.391654
2.088631	231.112147	4.396659
1.899592	247.180084	4.401664
2.139723	263.526846	4.406669
2.304022	269.908424	4.411674
2.336586	277.002106	4.416678
2.418158	271.713452	4.421683
2.298660	259.954659	4.426688
1.874946	260.194802	4.431693
2.477375	256.800176	4.436698
2.135838	261.390027	4.441702
2.207553	261.283301	4.446707
2.621396	269.435306	4.451712
1.967408	271.641367	4.456717
2.307461	269.131041	4.461722
2.134680	278.150401	4.466726
2.097606	273.406705	4.471731
2.033695	280.225094	4.476736
2.181946	275.430186	4.481741
2.334470	266.717628	4.486746
2.034906	268.466179	4.491750
2.098175	270.444139	4.496755
2.143481	271.500945	4.501760
2.393943	281.947809	4.506765
2.727555	290.157907	4.511770
2.571490	285.359516	4.516774
2.416698	273.039016	4.521779
2.413905	278.864743	4.526784
2.408948	279.336085	4.531789
2.584393	278.742717	4.536794
2.576410	290.833776	4.541798
2.712302	282.541333	4.546803
2.525935	284.166749	4.551808
2.402573	279.540745	4.556813
2.569780	287.751757	4.561818
2.674952	291.151305	4.566822
2.697674	289.654558	4.571827
2.268076	284.739450	4.576832
2.705186	289.614775	4.581837
2.716048	292.338274	4.586842
2.491518	311.338272	4.591846
2.738711	303.717081	4.596851
2.923422	297.078719	4.601856
2.755627	304.617830	4.606861
2.849185	293.318653	4.611866
3.059105	295.328967	4.616870
2.568537	281.909838	4.621875
2.532624	273.327150	4.626880
2.545869	296.580627	4.631885
3.076081	293.252615	4.636890
2.940990	303.680657	4.641894
2.836122	283.824248	4.646899
2.866501	281.916759	4.651904
2.674813	277.694179	4.656909
2.810261	280.786786	4.661914
2.751731	299.117540	4.666918
2.958797	294.580475	4.671923
2.595010	301.705466	4.676928
2.859327	305.390259	4.681933
2.793740	301.798991	4.686938
2.753018	319.688140	4.691942
3.163530	308.748900	4.696947
2.758882	308.397228	4.701952
2.761018	314.269315	4.706957
2.590048	306.475039	4.711962
3.033678	302.752085	4.716966
3.097722	302.916784	4.721971
3.325494	301.700833	4.726976
3.163332	315.893040	4.731981
3.171118	306.491053	4.736986
3.163141	311.537575	4.741990
3.324015	307.922223	4.746995
3.164737	310.389734	4.752000
3.059085	320.019615	4.757005
3.013825	312.808568	4.762010
3.017616	305.140854	4.767014
3.151493	302.140537	4.772019
3.127119	304.692269	4.777024
2.983639	310.243720	4.782029
3.166337	305.377582	4.787034
3.302072	306.436189	4.792038
3.165722	307.739558	4.797043
3.169282	304.259188	4.802048
2.975165	311.231172	4.807053
3.259884	311.345317	4.812058
3.078272	314.397489	4.817062
3.378976	305.639848	4.822067
3.171456	310.375849	4.827072
3.117457	310.491028	4.832077
3.290614	299.936244	4.837082
3.180906	312.193550	4.842086
3.313357	318.387624	4.847091
3.161700	307.870046	4.852096
2.971571	310.397526	4.857101
3.321340	311.394641	4.862106
2.823739	316.623479	4.867110
3.017645	311.400867	4.872115
2.935647	318.766131	4.877120
3.097460	339.626821	4.882125
3.292029	342.673932	4.887130
3.228286	341.563677	4.892134
3.506461	348.396095	4.897139
3.237203	343.232805	4.902144
3.616907	336.766973	4.907149
3.599408	341.533283	4.912154
3.590211	351.465911	4.917158
3.692349	344.435081	4.922163
3.713048	342.006834	4.927168
3.590292	341.737539	4.932173
3.903989	340.794878	4.937178
3.711351	335.931880	4.942182
3.337654	315.701394	4.947187
3.355710	323.671902	4.952192
3.703674	342.913597	4.957197
3.519239	340.969645	4.962202
3.321197	352.609340	4.967206
3.562591	353.936988	4.972211
3.954511	349.905661	4.977216
3.721294	349.449427	4.982221
3.758015	345.768192	4.987226
3.473850	346.082908	4.992230
3.638518	345.672874	4.997235
3.832080	342.891972	5.002240
3.557764	346.671102	5.007245
3.732338	346.600032	5.012250
3.417625	353.230679	5.017254
3.752698	354.113012	5.022259
3.623280	347.631039	5.027264
3.636447	343.984095	5.032269
3.869785	345.047854	5.037274
3.558892	353.884502	5.042278
3.924319	352.103270	5.047283
3.930713	350.244934	5.052288
3.623086	346.778592	5.057293
3.856067	345.825616	5.062298
3.721235	356.340085	5.067302
3.601910	348.153807	5.072307
3.697916	350.093598	5.077312
3.373977	351.838103	5.082317
3.703761	351.942024	5.087322
3.627704	354.620923	5.092326
3.715951	368.477085	5.097331
3.676762	372.052113	5.102336
3.700760	382.211136	5.107341
4.115208	374.904793	5.112346
3.979811	381.478327	5.117350
4.016743	373.479878	5.122355
4.476817	371.387160	5.127360
3.729551	377.097426	5.132365
4.062506	373.355486	5.137370
3.697181	377.850246	5.142374
3.682784	373.440608	5.147379
3.891979	364.719597	5.152384
4.179104	374.939238	5.157389
4.263004	369.801721	5.162394
4.067192	371.985993	5.167398
4.026471	374.523867	5.172403
4.060528	367.525219	5.177408
4.049664	378.385630	5.182413
4.103866	373.957133	5.187418
4.267060	375.461524	5.192422
3.915157	370.172196	5.197427
4.150483	370.781749	5.202432
4.143179	379.446381	5.207437
4.548877	373.408203	5.212442
4.138561	371.405548	5.217446
4.332111	375.358419	5.222451
4.152268	373.970986	5.227456
3.994467	378.835924	5.232461
4.112525	377.102560	5.237466
4.032279	377.334766	5.242470
4.107388	380.880015	5.247475
4.059810	390.291143	5.252480
4.095123	405.050639	5.257485
4.511954	407.084722	5.262490
4.226888	410.522475	5.267494
4.311386	405.916873	5.272499
4.682193	410.056881	5.277504
4.292561	405.333638	5.282509
4.523697	402.700822	5.287514
4.403580	406.906338	5.292518
4.664771	403.501292	5.297523
4.517943	401.812183	5.302528
4.529818	405.239441	5.307533
4.685187	392.380453	5.312538
4.487885	393.463036	5.317542
4.138014	392.606971	5.322547
4.344492	393.919881	5.327552
4.396049	397.496662	5.332557
4.591738	397.091158	5.337562
4.775674	409.056004	5.342566
4.563984	410.035987	5.347571
5.027400	400.004759	5.352576
4.432039	407.696027	5.357581
4.605632	396.801682	5.362586
4.362743	409.080330	5.367590
4.469522	408.286583	5.372595
4.448672	397.026010	5.377600
4.640003	407.060053	5.382605
4.424588	405.369672	5.387610
4.620000	405.062883	5.392614
4.541534	403.877113	5.397619
4.591521	406.795439	5.402624
4.160113	410.531333	5.407629
4.535561	402.361960	5.412634
4.476619	408.046858	5.417638
4.652666	413.739022	5.422643
4.849681	401.251626	5.427648
4.726931	409.765088	5.432653
4.795191	401.305189	5.437658
4.753921	404.995421	5.442662
4.486809	403.133036	5.447667
4.889846	421.592930	5.452672
4.876196	438.433020	5.457677
4.966659	428.786973	5.462682
4.815405	428.369063	5.467686
4.821450	429.277865	5.472691
4.900581	433.284628	5.477696
4.953274	439.937945	5.482701
4.733458	438.839122	5.487706
4.703755	442.111456	5.492710
5.116098	440.555502	5.497715
5.367242	431.910785	5.502720
4.644724	424.259091	5.507725
4.970288	429.640558	5.512730
4.756655	440.438092	5.517734
4.741682	432.103456	5.522739
4.997827	439.223730	5.527744
4.693690	437.660324	5.532749
4.791228	437.439601	5.537754
4.938783	440.577596	5.542758
5.017677	442.225408	5.547763
4.891868	431.392657	5.552768
4.957127	443.626815	5.557773
5.223355	443.623845	5.562778
4.987073	442.372838	5.567782
4.869442	436.895306	5.572787
4.967591	436.867479	5.577792
4.722297	445.594844	5.582797
5.094497	449.703650	5.587802
5.279365	464.733459	5.592806
5.321787	456.891929	5.597811
5.484503	443.773166	5.602816
5.189301	440.342437	5.607821
5.165873	434.106719	5.612826
4.992469	442.786854	5.617830
5.224353	447.335280	5.622835
5.638489	448.979676	5.627840
5.037885	443.509104	5.632845
5.334401	438.384507	5.637850
5.265558	442.921754	5.642854
5.190834	448.855955	5.647859
5.386307	447.820184	5.652864
5.549314	449.128261	5.657869
5.555766	447.341933	5.662874
5.127465	432.137886	5.667878
5.281179	436.815093	5.672883
5.556734	433.711366	5.677888
5.104682	445.860296	5.682893
5.426539	448.064826	5.687898
5.353509	461.824836	5.692902
5.352931	465.415396	5.697907
5.517655	464.762227	5.702912
5.040453	475.205200	5.707917
5.399331	462.567415	5.712922
5.397347	471.964136	5.717926
5.382770	464.948830	5.722931
5.478521	464.878775	5.727936
5.510825	474.924395	5.732941
5.613632	473.436865	5.737946
5.392336	461.468428	5.742950
5.440539	468.050669	5.747955
5.275108	466.886991	5.752960
5.329937	469.184881	5.757965
5.110189	471.660852	5.762970
5.073236	468.969803	5.767974
5.474041	491.132241	5.772979
5.820307	494.248195	5.777984
5.723309	499.555800	5.782989
5.519087	504.886294	5.787994
5.883872	493.052259	5.792998
5.773020	496.969333	5.798003
5.749551	482.320213	5.803008
5.607244	488.009868	5.808013
5.971176	496.655320	5.813018
5.518103	478.532529	5.818022
5.545996	474.636638	5.823027
5.817807	486.000695	5.828032
5.608412	493.733864	5.833037
5.621377	487.194707	5.838042
6.036062	498.242656	5.843046
5.882777	498.180687	5.848051
5.941511	490.085423	5.853056
5.988712	506.019192	5.858061
5.841284	507.636999	5.863066
5.726576	499.487765	5.868070
5.515053	500.372213	5.873075
5.995901	488.394244	5.878080
5.642855	503.377200	5.883085
5.982717	500.207951	5.888090
5.565755	495.478944	5.893094
5.356745	505.826415	5.898099
5.671989	500.465835	5.903104
5.930602	500.970895	5.908109
6.062059	492.846023	5.913114
6.015853	499.217956	5.918118
5.828813	499.459956	5.923123
5.811252	500.641250	5.928128
5.762413	497.094130	5.933133
5.917503	491.853416	5.938138
6.217999	509.958805	5.943142
6.138554	506.417738	5.948147
5.871970	499.914804	5.953152
5.942903	516.663220	5.958157
6.242762	517.827473	5.963162
6.053020	533.033445	5.968166
6.098797	536.256397	5.973171
6.198181	527.804497	5.978176
6.026898	541.103678	5.983181
6.276701	537.690621	5.988186
6.509569	525.721719	5.993190
6.249033	518.687521	5.998195
6.408433	501.481949	6.003200
6.011659	498.140648	6.008205
6.163652	497.112272	6.013210
6.141900	500.967427	6.018214
6.086321	497.879253	6.023219
5.732951	487.611043	6.028224
6.239522	518.358050	6.033229
6.594623	521.360853	6.038234
6.075825	514.883495	6.043238
6.244741	516.833336	6.048243
6.243437	500.738367	6.053248
6.015780	512.956359	6.058253
6.202441	514.240592	6.063258
6.284984	522.032587	6.068262
6.585219	521.667984	6.073267
6.473555	499.633984	6.078272
6.201611	497.574062	6.083277
6.315751	494.584672	6.088282
6.309385	494.952650	6.093286
6.074943	500.342810	6.098291
6.130995	492.474140	6.103296
5.978502	494.890827	6.108301
6.261361	495.591579	6.113306
6.354752	499.257362	6.118310
6.340958	501.766723	6.123315
6.403667	501.078545	6.128320
5.936623	496.927947	6.133325
5.948542	495.331536	6.138330
6.392235	499.201378	6.143334
5.775356	494.242621	6.148339
6.245668	492.953733	6.153344
5.982390	494.071521	6.158349
6.132938	497.632525	6.163354
6.218618	496.993233	6.168358
6.340435	500.596883	6.173363
6.110769	499.551983	6.178368
6.159021	505.738959	6.183373
6.248516	500.279203	6.188378
6.182079	501.491680	6.193382
5.723915	504.510749	6.198387
6.134694	516.041459	6.203392
6.102991	520.423587	6.208397
6.343639	526.564503	6.213402
6.082280	525.574579	6.218406
6.251951	527.980547	6.223411
6.136451	525.188235	6.228416
6.057329	528.992315	6.233421
6.290202	533.643813	6.238426
6.357813	531.923323	6.243430
6.391713	532.516312	6.248435
6.136643	512.564303	6.253440
6.018196	520.792154	6.258445
6.323369	523.179432	6.263450
6.427628	528.285191	6.268454
5.993819	513.907450	6.273459
6.503258	512.491507	6.278464
5.741664	508.240888	6.283469
5.974433	512.570535	6.288474
6.014880	512.996870	6.293478
6.204476	531.257406	6.298483
6.497511	534.128009	6.303488
6.113736	534.433372	6.308493
5.962486	531.128566	6.313498
6.355810	535.052344	6.318502
6.145650	526.675780	6.323507
6.380822	530.401370	6.328512
6.229438	521.545010	6.333517
6.371318	520.171383	6.338522
6.079001	525.637638	6.343526
6.344931	529.765050	6.348531
5.995022	520.168190	6.353536
5.846567	523.661098	6.358541
6.098431	521.921544	6.363546
6.223625	527.283535	6.368550
6.037672	532.592463	6.373555
6.420977	524.676886	6.378560
6.317692	521.442681	6.383565
6.337312	529.763513	6.388570
6.257008	530.241814	6.393574
5.960013	528.566902	6.398579
6.128116	528.071043	6.403584
6.300602	532.926724	6.408589
6.338281	526.834182	6.413594
6.230450	537.523881	6.418598
6.253792	531.731302	6.423603
6.357595	522.977925	6.428608
6.061159	522.054986	6.433613
5.900604	525.815321	6.438618
6.241927	521.391728	6.443622
6.127520	527.176236	6.448627
6.092885	529.766410	6.453632
6.235985	524.146606	6.458637
6.101799	531.281042	6.463642
6.419049	530.715885	6.468646
6.079345	530.438506	6.473651
6.299891	525.308502	6.478656
5.528578	530.668777	6.483661
6.454287	527.350411	6.488666
6.285120	528.171013	6.493670
6.352754	531.051510	6.498675
6.451613	531.389830	6.503680
6.504794	535.384142	6.508685
6.072490	511.851929	6.513690
6.174090	507.875940	6.518694
6.076350	516.226460	6.523699
6.248202	520.443254	6.528704
6.116048	516.503998	6.533709
6.221572	521.292616	6.538714
6.146681	532.595716	6.543718
6.143224	529.515875	6.548723
6.494910	519.143914	6.553728
5.973777	518.764558	6.558733
5.934307	523.883855	6.563738
6.463790	529.191133	6.568742
6.356496	527.555258	6.573747
6.210482	517.116921	6.578752
6.091385	515.617785	6.583757
6.126103	507.617660	6.588762
6.435172	522.486254	6.593766
6.019598	517.732146	6.598771
6.247166	513.793510	6.603776
6.291866	509.375626	6.608781
6.367438	504.066179	6.613786
6.360811	493.957620	6.618790
5.915296	499.396348	6.623795
6.420623	496.696010	6.628800
6.013005	499.391950	6.633805
5.906596	492.419268	6.638810
6.033305	511.954157	6.643814
6.239150	514.868599	6.648819
6.546671	518.333162	6.653824
6.008030	508.666918	6.658829
6.029507	495.627742	6.663834
6.209669	516.031553	6.668838
6.183604	527.540481	6.673843
6.417990	514.550296	6.678848
5.950095	517.924021	6.683853
5.918911	522.959456	6.688858
6.486701	526.343230	6.693862
6.391447	523.893701	6.698867
6.202533	508.427140	6.703872
6.267944	509.559569	6.708877
5.918976	502.215398	6.713882
6.308442	511.023580	6.718886
6.115066	520.865057	6.723891
6.194249	510.404628	6.728896
6.445774	523.727318	6.733901
6.094606	509.483507	6.738906
6.095345	504.842016	6.743910
5.869743	516.344904	6.748915
6.518259	518.925947	6.753920
6.296222	522.788620	6.758925
6.356148	518.483656	6.763930
6.354157	499.112955	6.768934
6.141082	500.429045	6.773939
5.855501	496.168475	6.778944
6.055032	513.606411	6.783949
6.131915	519.740895	6.788954
6.375930	526.536424	6.793958
5.999205	525.753077	6.798963
6.449918	532.416893	6.803968
6.326300	528.334727	6.808973
6.402207	508.128403	6.813978
6.171114	506.367789	6.818982
5.794534	499.929839	6.823987
6.347140	492.424337	6.828992
5.854391	505.477160	6.833997
6.133342	519.772928	6.839002
6.189419	526.095176	6.844006
6.000661	529.098843	6.849011
6.267490	528.347459	6.854016
6.326317	537.218894	6.859021
6.276970	528.364775	6.864026
6.528117	522.116114	6.869030
6.034131	515.776930	6.874035
6.058171	502.372047	6.879040
6.181556	523.744342	6.884045
6.528065	509.066689	6.889050
6.068496	508.618924	6.894054
5.749599	512.309174	6.899059
6.380477	515.874115	6.904064
6.344522	528.937749	6.909069
6.267127	518.932853	6.914074
6.117830	512.029229	6.919078
6.103023	524.866758	6.924083
6.190796	515.141179	6.929088
6.116708	534.661197	6.934093
6.668715	522.149848	6.939098
6.547040	509.366833	6.944102
6.243669	509.838066	6.949107
6.526167	496.857098	6.954112
6.141207	501.356723	6.959117
6.083790	500.093852	6.964122
6.002061	499.374535	6.969126
5.730028	498.090370	6.974131
6.037246	501.053736	6.979136
5.699859	503.341986	6.984141
6.379330	518.496558	6.989146
6.479203	523.053448	6.994150
6.183597	517.514386	6.999155
6.335486	496.978566	7.004160
6.079796	499.551269	7.009165
6.101355	500.776408	7.014170
6.104713	496.962129	7.019174
6.380037	516.595751	7.024179
6.437757	500.923182	7.029184
6.321283	498.966969	7.034189
6.639751	490.642207	7.039194
6.515476	489.315419	7.044198
6.176547	501.772652	7.049203
6.516114	489.618566	7.054208
6.328845	494.043222	7.059213
6.288872	497.846731	7.064218
6.151744	494.569195	7.069222
6.063895	499.444295	7.074227
6.435453	497.015151	7.079232
6.186350	498.879892	7.084237
6.059893	505.495216	7.089242
6.288044	494.597885	7.094246
5.979245	503.613061	7.099251
6.346857	492.294406	7.104256
6.064724	501.036388	7.109261
6.012597	499.112736	7.114266
6.145989	490.613388	7.119270
6.247219	492.155877	7.124275
6.318504	490.623638	7.129280
6.262983	490.325643	7.134285
6.477791	493.250437	7.139290
6.611101	493.190936	7.144294
6.070233	500.488215	7.149299
6.228746	491.179954	7.154304
5.883512	491.447558	7.159309
6.219919	495.433046	7.164314
6.567902	493.229616	7.169318
6.250906	497.557351	7.174323
6.060981	484.902681	7.179328
5.750333	494.001040	7.184333
5.830672	496.818055	7.189338
6.315139	484.954341	7.194342
6.217308	500.956325	7.199347
6.375699	492.154262	7.204352
6.149569	490.227654	7.209357
6.107521	494.457167	7.214362
6.091557	486.984055	7.219366
6.254213	500.176593	7.224371
6.414627	486.870900	7.229376
6.400429	500.544437	7.234381
5.975636	500.484606	7.239386
6.336210	491.515463	7.244390
6.278866	499.734566	7.249395
6.210262	502.151768	7.254400
6.199469	497.555603	7.259405
6.066040	500.185813	7.264410
6.225043	482.780225	7.269414
5.949287	500.886701	7.274419
6.186709	491.771199	7.279424
6.182847	494.739899	7.284429
6.114072	493.259073	7.289434
6.558679	494.145773	7.294438
6.126301	497.105315	7.299443
6.308300	490.264060	7.304448
6.268398	493.639921	7.309453
6.305133	494.893330	7.314458
6.677191	498.422980	7.319462
5.976061	499.287270	7.324467
5.938902	483.478281	7.329472
5.884072	494.123455	7.334477
6.066870	492.467963	7.339482
6.161677	495.746725	7.344486
5.754049	503.095746	7.349491
6.314177	497.943658	7.354496
5.962930	497.248251	7.359501
6.260179	499.010086	7.364506
6.596802	499.310018	7.369510
6.600312	503.580733	7.374515
6.393988	494.348280	7.379520
6.419195	498.679733	7.384525
6.146048	497.484358	7.389530
5.966747	489.197230	7.394534
6.084429	494.428828	7.399539
6.473732	491.014586	7.404544
6.734139	489.761445	7.409549
5.909237	485.663597	7.414554
6.123906	477.125538	7.419558
5.871591	469.468776	7.424563
6.069705	480.258737	7.429568
6.164210	484.795588	7.434573
6.274848	491.747773	7.439578
6.566972	490.721452	7.444582
5.998625	487.213791	7.449587
6.090872	481.261420	7.454592
6.084077	485.636453	7.459597
5.969645	491.939167	7.464602
6.112278	495.340253	7.469606
5.943916	510.609167	7.474611
6.061465	503.891851	7.479616
5.905804	500.236715	7.484621
5.864139	497.329959	7.489626
6.138843	507.828612	7.494630
6.043017	505.285444	7.499635
6.391198	495.748038	7.504640
6.300234	497.829320	7.509645
5.989168	500.367385	7.514650
6.285805	487.226408	7.519654
6.174233	491.273844	7.524659
6.351910	492.900962	7.529664
6.181117	497.462606	7.534669
6.000846	502.956280	7.539674
6.089888	495.144702	7.544678
5.873542	505.734735	7.549683
6.514138	493.135722	7.554688
6.097572	504.113332	7.559693
6.204802	491.288282	7.564698
6.365624	487.594751	7.569702
6.313707	498.144130	7.574707
6.465777	487.247169	7.579712
6.322608	497.598137	7.584717
6.089596	494.268200	7.589722
6.709846	494.431375	7.594726
6.293062	496.467152	7.599731
6.402036	494.268964	7.604736
6.361112	493.756412	7.609741
6.455816	495.432988	7.614746
6.238295	486.219364	7.619750
5.852438	486.643278	7.624755
6.084909	480.870157	7.629760
6.330225	485.694818	7.634765
5.963322	498.808889	7.639770
6.181631	488.914100	7.644774
6.383462	497.750386	7.649779
6.873264	488.836018	7.654784
6.298406	476.325613	7.659789
5.768436	476.545661	7.664794
6.480174	465.193720	7.669798
6.402122	466.097505	7.674803
6.496687	449.598546	7.679808
6.183053	456.507109	7.684813
5.911179	460.576543	7.689818
6.118102	462.976727	7.694822
6.007197	463.136062	7.699827
6.225376	457.275725	7.704832
6.171750	453.145283	7.709837
5.959307	469.173319	7.714842
6.017642	458.165208	7.719846
6.053965	473.473402	7.724851
6.368210	484.176053	7.729856
6.630895	483.947913	7.734861
6.352029	483.583300	7.739866
6.432521	472.898107	7.744870
6.108427	473.751071	7.749875
6.299930	464.981231	7.754880
6.115932	465.088732	7.759885
6.140894	468.192371	7.764890
6.370465	466.495588	7.769894
6.072935	471.546499	7.774899
5.952148	470.050805	7.779904
6.112025	461.394741	7.784909
6.034045	470.503498	7.789914
6.209469	456.037554	7.794918
5.944150	468.241619	7.799923
6.021250	467.012520	7.804928
6.412252	473.495174	7.809933
6.148104	471.614135	7.814938
6.248621	463.044468	7.819942
5.935618	468.517484	7.824947
6.180360	481.404746	7.829952
5.905275	491.300387	7.834957
5.818060	489.619158	7.839962
6.361775	491.107909	7.844966
6.199530	496.949268	7.849971
6.281852	505.074993	7.854976
6.029737	498.072761	7.859981
5.998033	495.902407	7.864986
6.094026	497.385377	7.869990
6.070644	506.107010	7.874995
6.003932	493.027383	7.880000
6.287479	496.044003	7.885005
5.942460	500.781715	7.890010
6.150276	492.235705	7.895014
6.010025	500.884728	7.900019
5.741882	501.861632	7.905024
5.833310	507.381752	7.910029
5.797643	505.779801	7.915034
6.303717	512.498971	7.920038
6.526741	533.032266	7.925043
6.510202	515.878704	7.930048
6.449709	503.767965	7.935053
6.007421	503.996582	7.940058
6.537157	502.844477	7.945062
6.154028	507.607842	7.950067
6.255403	496.618428	7.955072
6.568198	501.524866	7.960077
6.162934	504.971691	7.965082
6.583371	487.320729	7.970086
6.017652	503.173650	7.975091
6.288792	502.924376	7.980096
6.274976	499.711472	7.985101
6.302033	494.364280	7.990106
6.485489	493.630255	7.995110
6.157145	501.720972	8.000115
6.325554	489.144545	8.005133
6.422301	499.477862	8.010150
6.119581	507.314129	8.015168
6.546221	498.939997	8.020186
6.569432	493.751156	8.025203
5.847297	481.789777	8.030221
6.105106	474.063847	8.035238
6.125909	495.486701	8.040256
6.400082	494.382782	8.045274
6.031065	498.373997	8.050291
5.989896	499.831372	8.055309
6.219914	504.551089	8.060326
5.890736	502.878428	8.065344
6.090535	498.365018	8.070362
6.125271	509.044216	8.075379
5.999899	508.112555	8.080397
6.018564	507.100352	8.085414
5.989819	508.072830	8.090432
6.154102	499.802572	8.095450
5.719918	499.991068	8.100467
6.041912	518.126903	8.105485
6.090630	524.524959	8.110502
6.108910	536.057828	8.115520
6.533286	536.217134	8.120538
6.779603	535.219787	8.125555
6.470084	524.332096	8.130573
6.235352	521.807827	8.135590
6.266382	530.448621	8.140608
6.469700	532.564678	8.145626
6.404224	540.711062	8.150643
6.198692	532.696894	8.155661
6.473561	535.801626	8.160678
6.431757	539.816220	8.165696
6.461188	525.362008	8.170714
6.371078	511.349229	8.175731
5.972061	516.141227	8.180749
6.503248	526.855542	8.185766
6.390655	532.236292	8.190784
6.675005	528.949338	8.195802
6.426704	518.758748	8.200819
6.119937	503.382345	8.205837
6.186704	503.324904	8.210854
6.308738	535.785988	8.215872
6.433714	531.097570	8.220890
6.344711	539.326976	8.225907
6.380381	534.877543	8.230925
6.507394	528.696764	8.235942
6.559230	531.327439	8.240960
6.447338	535.008387	8.245978
6.399622	534.743739	8.250995
6.656688	537.711468	8.256013
6.654774	524.504488	8.261030
6.359765	532.457200	8.266048
6.771388	532.962689	8.271066
6.454514	523.172205	8.276083
6.204814	515.578718	8.281101
6.541714	524.526708	8.286118
6.428143	543.668298	8.291136
6.685612	533.427604	8.296154
6.651276	531.868112	8.301171
6.227239	514.448266	8.306189
6.870270	515.973628	8.311206
6.345543	518.431687	8.316224
6.167037	520.023019	8.321242
6.194788	531.876341	8.326259
6.143846	531.715567	8.331277
6.508499	535.292011	8.336294
6.208437	533.678497	8.341312
6.400113	536.370066	8.346330
6.726967	551.290787	8.351347
6.457380	542.572703	8.356365
6.862031	527.489856	8.361382
6.558974	535.833836	8.366400
6.302400	534.351300	8.371418
6.531984	536.219324	8.376435
6.499589	534.748875	8.381453
6.296608	537.861482	8.386470
6.254621	536.252079	8.391488
6.795816	538.821403	8.396506
6.654642	539.344423	8.401523
6.573758	538.303627	8.406541
6.692333	539.166679	8.411558
6.153721	543.048007	8.416576
6.431548	535.929123	8.421594
6.537598	542.054522	8.426611
6.505046	560.596535	8.431629
6.894960	565.130748	8.436646
6.559276	563.746146	8.441664
6.793402	554.906456	8.446682
6.862030	563.989438	8.451699
6.396762	549.875768	8.456717
6.936700	553.233833	8.461734
6.336236	552.593032	8.466752
6.738500	557.232276	8.471770
6.991761	561.980049	8.476787
6.571982	551.023990	8.481805
6.650023	549.194132	8.486822
6.447609	544.749282	8.491840
6.830082	560.239108	8.496858
6.917865	562.784511	8.501875
6.944518	562.906536	8.506893
6.869639	541.284627	8.511910
6.724263	542.911812	8.516928
6.534967	539.959965	8.521946
6.671146	535.362007	8.526963
6.597021	544.173165	8.531981
6.823144	548.893934	8.536998
6.620266	567.476955	8.542016
6.877100	566.332205	8.547034
7.100035	555.312621	8.552051
6.611333	551.027375	8.557069
6.833881	541.231800	8.562087
6.478743	538.863284	8.567104
6.671535	553.898524	8.572122
7.010390	566.105052	8.577139
6.899770	566.262997	8.582157
6.997910	553.117963	8.587175
6.577089	550.757961	8.592192
6.548916	553.892801	8.597210
6.876045	560.902402	8.602227
6.672983	567.006562	8.607245
6.943069	564.920309	8.612263
7.238177	565.427773	8.617280
6.856870	560.766692	8.622298
6.734170	550.362775	8.627315
6.907496	552.632414	8.632333
7.136240	563.748784	8.637351
6.844480	552.584331	8.642368
6.802394	540.918140	8.647386
7.072654	536.176727	8.652403
6.919834	538.876134	8.657421
6.742391	529.287344	8.662439
6.611295	534.156233	8.667456
6.621637	557.078243	8.672474
6.957145	556.974135	8.677491
6.699203	570.320369	8.682509
7.110021	558.970871	8.687527
7.221600	574.102645	8.692544
6.788509	566.092681	8.697562
6.899837	563.901820	8.702579
6.496082	575.872101	8.707597
6.976615	565.421231	8.712615
6.956681	573.295737	8.717632
6.770821	574.546977	8.722650
6.829535	565.481226	8.727667
6.930588	566.102118	8.732685
7.118642	571.253579	8.737703
7.266565	563.054496	8.742720
7.022115	569.671777	8.747738
7.181323	567.338547	8.752755
6.614040	557.885749	8.757773
6.777900	564.449782	8.762791
6.976925	573.071245	8.767808
7.096288	567.957789	8.772826
7.223241	572.234387	8.777843
6.722567	576.200970	8.782861
7.175745	569.881129	8.787879
7.095198	572.793756	8.792896
6.713868	573.590586	8.797914
7.174330	564.367763	8.802931
7.026057	576.763226	8.807949
6.944896	561.787959	8.812967
6.960076	566.695032	8.817984
6.919987	576.243043	8.823002
7.513923	569.393037	8.828019
6.914236	573.792326	8.833037
7.043772	570.805982	8.838055
7.160129	573.755093	8.843072
7.023632	568.308440	8.848090
7.062623	563.450799	8.853107
6.864688	570.398937	8.858125
6.830834	570.499882	8.863143
6.976361	572.149759	8.868160
7.023816	572.329556	8.873178
7.380306	587.160173	8.878195
7.105832	589.034711	8.883213
7.149242	575.568427	8.888231
7.199092	563.667324	8.893248
7.010039	573.263424	8.898266
7.602613	581.075282	8.903283
7.566013	577.843041	8.908301
7.637534	576.164643	8.913319
7.364269	571.422877	8.918336
7.114556	580.273367	8.923354
7.412205	565.449920	8.928371
7.292001	570.560701	8.933389
7.366148	567.136118	8.938407
6.984536	556.558355	8.943424
7.398091	560.995350	8.948442
7.451880	563.538509	8.953459
7.484367	566.303488	8.958477
7.095381	570.247244	8.963495
7.054430	569.459659	8.968512
7.179347	571.239318	8.973530
7.256408	567.386722	8.978547
6.934027	568.649939	8.983565
7.230667	561.734411	8.988583
7.349345	570.255996	8.993600
7.110800	568.565367	8.998618
7.725242	560.148489	9.003635
7.490660	565.369542	9.008653
7.070422	571.692530	9.013671
7.422486	570.743806	9.018688
7.320896	573.166840	9.023706
7.579550	573.092977	9.028723
7.351445	572.965870	9.033741
7.004060	571.288540	9.038759
7.568952	575.751460	9.043776
7.085271	573.267029	9.048794
7.086140	568.120836	9.053811
6.975129	573.177344	9.058829
7.296861	568.749226	9.063847
7.175943	569.200787	9.068864
7.250611	566.580396	9.073882
7.366620	569.101245	9.078899
7.100844	571.829402	9.083917
7.298531	583.436329	9.088935
7.410110	591.072939	9.093952
7.067399	604.799358	9.098970
7.762154	602.115251	9.103987
7.437547	607.546685	9.109005
7.406480	600.395661	9.114023
7.798137	599.262045	9.119040
7.228736	605.136745	9.124058
7.755027	591.857593	9.129075
7.598840	597.585523	9.134093
7.222355	573.337111	9.139111
7.295594	577.667878	9.144128
7.466744	598.225677	9.149146
7.707983	597.588199	9.154163
7.494282	606.414041	9.159181
7.467278	610.170314	9.164199
7.679050	603.626672	9.169216
7.190043	602.671959	9.174234
7.944859	601.482928	9.179251
7.276891	588.614522	9.184269
7.338932	601.299173	9.189287
7.640834	595.820068	9.194304
7.197139	608.181805	9.199322
7.398158	607.882068	9.204339
7.344901	605.806050	9.209357
7.485270	609.691289	9.214375
7.696271	608.301779	9.219392
7.282363	613.165756	9.224410
7.526951	599.160461	9.229427
7.490560	604.700456	9.234445
7.480937	605.565450	9.239463
7.841649	606.665556	9.244480
7.524491	598.578507	9.249498
7.418551	599.777934	9.254515
7.672793	606.868125	9.259533
7.638970	603.412992	9.264551
7.758954	592.414761	9.269568
7.413587	604.742104	9.274586
7.429848	598.124548	9.279603
7.295612	603.126057	9.284621
7.510158	611.035764	9.289639
7.812458	607.984782	9.294656
7.239750	609.140647	9.299674
7.572217	605.034343	9.304691
7.938509	625.747647	9.309709
7.574578	621.707450	9.314727
7.792207	618.727965	9.319744
7.502656	626.221975	9.324762
7.641976	634.407127	9.329779
8.118720	631.296941	9.334797
7.898450	632.692851	9.339815
8.000906	616.835996	9.344832
7.430582	620.280299	9.349850
7.780755	605.134356	9.354867
7.599742	603.664496	9.359885
7.557973	609.060117	9.364903
7.656288	610.002113	9.369920
7.703295	628.243649	9.374938
7.786571	626.297371	9.379955
7.934293	636.742410	9.384973
7.823657	632.139038	9.389991
7.989699	625.193931	9.395008
7.572555	616.620705	9.400026
7.497195	617.574533	9.405043
7.454487	626.307902	9.410061
7.478664	637.676493	9.415079
7.459484	636.116055	9.420096
7.555103	640.983849	9.425114
7.762374	628.980648	9.430131
7.715833	631.400086	9.435149
7.598659	636.543259	9.440167
7.879771	630.033397	9.445184
7.719843	638.877123	9.450202
7.619426	632.185967	9.455219
8.073656	634.640977	9.460237
7.685948	645.417191	9.465255
7.932999	647.933675	9.470272
8.014445	662.953997	9.475290
8.190891	647.420664	9.480307
8.300781	635.450906	9.485325
8.139885	637.946365	9.490343
8.238217	632.643862	9.495360
7.677692	633.678427	9.500378
7.735847	629.765564	9.505395
7.882300	631.290105	9.510413
8.138538	629.456515	9.515431
8.274968	630.698087	9.520448
8.229192	638.816654	9.525466
8.156475	633.851513	9.530483
7.852613	633.046442	9.535501
7.857802	633.635773	9.540519
8.064227	631.685636	9.545536
7.813900	632.694028	9.550554
7.774100	637.659045	9.555571
8.001748	637.201364	9.560589
7.956042	635.325653	9.565607
7.895245	626.653650	9.570624
8.041129	632.069383	9.575642
7.849081	635.199095	9.580659
7.864332	629.632022	9.585677
7.703732	642.684263	9.590695
8.129978	649.264524	9.595712
8.272403	662.952781	9.600730
7.977699	645.880639	9.605747
8.092883	647.098173	9.610765
7.966383	657.920506	9.615783
8.178263	651.372890	9.620800
7.955778	653.095527	9.625818
8.190184	657.708468	9.630835
8.138260	663.499860	9.635853
8.069408	667.350079	9.640871
8.228657	664.318445	9.645888
8.144366	660.145715	9.650906
8.090919	662.185222	9.655923
8.481491	656.796919	9.660941
7.639055	657.257339	9.665959
8.436513	661.950654	9.670976
8.406330	663.346977	9.675994
8.418230	657.275755	9.681011
8.149617	635.596431	9.686029
8.127064	639.305913	9.691047
8.187129	643.503653	9.696064
8.254429	636.420964	9.701082
8.256634	642.807285	9.706099
8.230653	637.357660	9.711117
8.399926	641.305439	9.716135
8.174786	629.667919	9.721152
7.931814	640.901235	9.726170
8.261650	649.872514	9.731187
8.558542	657.090303	9.736205
8.282871	653.600015	9.741223
8.437857	633.583908	9.746240
8.267363	635.471151	9.751258
8.016065	636.834013	9.756275
8.251793	630.672984	9.761293
8.146789	630.294009	9.766311
8.336178	644.907880	9.771328
8.627413	652.243526	9.776346
8.236687	652.122089	9.781363
8.281857	638.221825	9.786381
7.980338	635.460974	9.791399
8.281675	660.343093	9.796416
8.338169	665.645694	9.801434
8.273306	670.788877	9.806451
8.673018	667.181234	9.811469
8.340825	662.734613	9.816487
8.389510	665.196552	9.821504
8.686162	667.675300	9.826522
8.276734	644.219389	9.831539
8.536590	648.387195	9.836557
8.285132	655.893020	9.841575
8.379074	650.862876	9.846592
8.434996	653.523209	9.851610
8.275368	658.563583	9.856627
8.849899	662.621413	9.861645
8.280807	660.366257	9.866663
8.308273	662.605344	9.871680
8.341292	668.551954	9.876698
8.551635	666.725566	9.881715
8.649743	660.966425	9.886733
8.670001	668.863849	9.891751
8.473673	655.512585	9.896768
8.202654	656.933436	9.901786
7.926473	663.147374	9.906803
8.530634	667.760108	9.911821
8.379780	669.233498	9.916839
8.532702	666.857596	9.921856
8.341948	668.981256	9.926874
8.434238	665.658365	9.931891
8.606774	653.338081	9.936909
8.459972	660.951374	9.941927
8.310568	661.504500	9.946944
8.410917	657.451580	9.951962
8.534886	658.756632	9.956979
8.845147	654.488648	9.961997
8.682502	663.142692	9.967015
8.522495	658.070745	9.972032
9.039103	659.948534	9.977050
8.612860	662.127723	9.982067
8.686173	662.839231	9.987085
8.322891	662.598295	9.992103
8.478276	662.869073	9.997120
8.742500	654.837285	10.002138
8.486349	663.392647	10.007155
8.588119	650.649071	10.012173
8.557149	659.138009	10.017191
8.865151	659.570510	10.022208
8.632733	661.350695	10.027226
8.430627	668.235792	10.032243
8.796007	659.873884	10.037261
8.340931	663.799869	10.042279
8.484381	660.305132	10.047296
8.499072	672.013882	10.052314
8.580327	691.628480	10.057331
8.883522	685.947960	10.062349
8.884444	689.175642	10.067367
8.988654	695.221096	10.072384
8.979683	676.598540	10.077402
8.574775	673.722528	10.082419
8.717971	681.777149	10.087437
8.627195	692.851450	10.092455
8.594885	686.945008	10.097472
9.134589	688.276095	10.102490
8.359861	696.341004	10.107507
8.699069	692.390246	10.112525
8.920414	693.031575	10.117543
9.184731	698.255681	10.122560
8.856710	697.853009	10.127578
8.828026	700.486418	10.132595
8.868854	697.630284	10.137613
8.894563	701.574688	10.142631
8.618931	695.154238	10.147648
9.138647	693.439205	10.152666
8.830269	696.444501	10.157683
8.998292	701.966428	10.162701
9.130787	698.486487	10.167719
8.851076	684.052613	10.172736
8.892135	684.673800	10.177754
8.882036	691.681433	10.182771
8.824537	685.506345	10.187789
8.792191	696.400115	10.192807
9.153546	701.951835	10.197824
8.994983	694.213648	10.202842
9.101847	697.036409	10.207859
8.929334	688.585221	10.212877
8.815343	696.241127	10.217895
8.900613	689.999090	10.222912
9.014278	688.575694	10.227930
8.610268	690.079984	10.232947
8.903386	689.781136	10.237965
8.916922	689.364815	10.242983
8.807883	695.257797	10.248000
8.801121	702.472745	10.253018
8.913406	701.704657	10.258035
9.054604	692.374401	10.263053
9.202374	704.663072	10.268071
8.697300	708.429641	10.273088
8.700997	699.796914	10.278106
8.952580	704.540088	10.283123
9.156989	695.439506	10.288141
9.140337	692.122446	10.293159
8.586742	695.888780	10.298176
9.348703	699.831335	10.303194
9.264011	707.587507	10.308211
9.296461	699.564551	10.313229
9.412079	695.502006	10.318247
9.093166	703.305229	10.323264
9.284314	693.566329	10.328282
9.296939	698.197899	10.333299
9.100063	705.928949	10.338317
9.201749	705.273633	10.343335
9.328995	707.833587	10.348352
9.588248	697.287783	10.353370
9.425930	705.285141	10.358387
9.228818	701.254698	10.363405
9.522637	697.183116	10.368423
9.239809	703.416673	10.373440
9.274416	701.216256	10.378458
8.935345	697.619928	10.383475
9.085418	694.776805	10.388493
8.548930	696.385705	10.393511
8.537585	696.988406	10.398528
9.078808	705.745982	10.403546
9.256211	720.658743	10.408563
9.677532	724.182937	10.413581
9.706228	724.081016	10.418599
9.340029	702.421301	10.423616
9.512693	696.288405	10.428634
9.017880	697.584910	10.433651
9.220899	697.607657	10.438669
9.129129	695.994277	10.443687
9.161817	700.049723	10.448704
9.546660	707.810814	10.453722
9.181884	706.002498	10.458739
9.376164	718.948008	10.463757
9.705156	715.805976	10.468775
9.427273	709.125277	10.473792
9.485715	707.171292	10.478810
9.231557	696.599096	10.483827
9.382911	700.746303	10.488845
9.316706	698.353537	10.493863
8.922142	716.323437	10.498880
9.618039	713.514720	10.503898
9.586446	736.344339	10.508915
9.704354	736.467789	10.513933
9.616084	718.547253	10.518951
9.305118	704.740547	10.523968
9.609789	704.320107	10.528986
9.316321	701.956707	10.534003
9.496165	712.056733	10.539021
9.408143	711.302131	10.544039
9.286908	731.529018	10.549056
9.862739	734.259954	10.554074
9.672983	728.013054	10.559091
9.240621	725.746663	10.564109
9.641654	725.085080	10.569127
9.319454	735.794607	10.574144
9.484593	730.696744	10.579162
9.602664	736.154125	10.584179
9.446252	741.103841	10.589197
9.577687	724.718877	10.594215
9.733530	734.504012	10.599232
9.670695	732.107140	10.604250
9.767372	729.792902	10.609267
9.407127	730.528967	10.614285
9.447955	731.021855	10.619303
9.599100	739.153138	10.624320
9.678330	729.623290	10.629338
9.562923	729.696798	10.634355
9.555232	727.154582	10.639373
9.731645	728.418280	10.644391
9.334783	733.762122	10.649408
9.586725	730.786382	10.654426
9.859287	727.028137	10.659443
9.748553	726.717034	10.664461
9.820801	729.999839	10.669479
9.853915	727.189856	10.674496
9.754266	724.437290	10.679514
9.784473	728.106169	10.684531
9.588101	736.508372	10.689549
9.983368	729.592185	10.694567
9.819424	734.789589	10.699584
9.720457	728.452462	10.704602
9.808952	729.125241	10.709619
9.825869	727.891869	10.714637
9.815950	729.205713	10.719655
9.745314	730.814241	10.724672
9.747607	734.355861	10.729690
9.980496	733.615435	10.734707
9.727830	737.048497	10.739725
9.812620	728.025575	10.744743
9.680298	725.180394	10.749760
9.865715	725.081653	10.754778
9.652917	730.143846	10.759795
9.509118	734.482450	10.764813
10.039210	735.549006	10.769831
9.840611	736.640566	10.774848
9.635007	727.773600	10.779866
9.724836	734.558024	10.784883
9.275990	727.445418	10.789901
9.817609	735.605340	10.794919
9.844458	754.887315	10.799936
10.015168	746.133997	10.804954
9.693207	754.407409	10.809971
9.831945	770.652534	10.814989
10.261974	756.519544	10.820007
10.025512	771.441048	10.825024
10.111105	758.490625	10.830042
10.053524	766.792307	10.835059
9.803371	764.663050	10.840077
10.187452	758.908876	10.845095
9.933711	773.378938	10.850112
10.306964	764.734188	10.855130
10.418558	765.015369	10.860147
10.051977	759.402430	10.865165
9.610869	746.623877	10.870183
10.109702	748.645952	10.875200
9.902853	756.814481	10.880218
10.355554	765.900906	10.885235
10.220065	761.953545	10.890253
10.231152	761.739586	10.895271
9.959886	754.281435	10.900288
10.121694	762.365298	10.905306
10.064530	758.552204	10.910323
10.024172	757.185408	10.915341
10.615888	762.804509	10.920359
10.062915	755.574494	10.925376
10.152388	749.024667	10.930394
10.084952	741.637882	10.935411
9.836123	755.842167	10.940429
9.951235	751.589938	10.945447
9.711694	762.726323	10.950464
9.882182	757.497651	10.955482
10.417334	759.672367	10.960499
10.337073	764.859467	10.965517
10.626372	758.071045	10.970535
10.331172	772.044848	10.975552
10.490028	757.011930	10.980570
10.421017	757.594657	10.985587
10.307217	763.842766	10.990605
10.404033	752.547094	10.995623
10.430642	759.912833	11.000640
10.480303	760.577477	11.005658
10.397992	767.117601	11.010675
10.248111	764.882374	11.015693
10.564704	761.869939	11.020711
10.337797	742.060625	11.025728
10.156834	742.902821	11.030746
10.147104	743.450535	11.035763
10.354263	763.836065	11.040781
10.188614	762.525841	11.045799
10.216287	762.379604	11.050816
10.241990	760.273167	11.055834
10.698243	756.962030	11.060851
10.061295	761.505133	11.065869
10.382442	764.510520	11.070887
10.337206	759.051837	11.075904
10.296690	760.794350	11.080922
10.237165	763.270680	11.085939
10.035129	765.104110	11.090957
10.463606	760.180729	11.095975
10.492775	763.986395	11.100992
10.266651	752.239502	11.106010
10.261419	757.614165	11.111027
10.593144	756.873119	11.116045
10.652161	765.531062	11.121063
10.369673	754.981234	11.126080
10.132918	752.804093	11.131098
10.568269	767.287590	11.136115
10.675350	780.467658	11.141133
10.591011	784.179533	11.146151
10.735934	793.129156	11.151168
10.555324	776.052936	11.156186
10.521511	763.651387	11.161203
10.317672	771.406061	11.166221
10.836067	776.962510	11.171239
10.788629	789.670955	11.176256
10.711507	779.099307	11.181274
10.650149	752.457017	11.186291
10.382917	767.113548	11.191309
10.468169	770.945754	11.196327
10.699187	786.438251	11.201344
10.693723	792.643629	11.206362
10.486994	774.475336	11.211379
10.536445	798.902565	11.216397
10.782093	785.211478	11.221415
10.824628	789.498376	11.226432
10.783125	786.196828	11.231450
10.822743	787.566643	11.236467
10.779398	787.375870	11.241485
10.719761	791.935580	11.246503
11.014798	786.182363	11.251520
10.584511	792.089212	11.256538
10.653619	786.733231	11.261555
10.472988	791.218888	11.266573
10.892927	786.793737	11.271591
10.756064	790.986727	11.276608
10.724809	794.485494	11.281626
10.916856	789.287886	11.286643
10.611582	791.412022	11.291661
10.667544	790.186352	11.296679
10.708344	793.433828	11.301696
10.640254	788.314336	11.306714
10.975797	789.443425	11.311731
10.938033	796.585996	11.316749
11.204178	790.751345	11.321767
10.879384	790.716228	11.326784
10.578363	797.720119	11.331802
11.131447	787.079537	11.336819
10.978915	789.975582	11.341837
10.942244	796.258961	11.346855
10.850708	788.867483	11.351872
10.816362	797.208638	11.356890
11.307176	783.477348	11.361907
11.138286	788.991321	11.366925
10.947454	788.518293	11.371943
11.144644	781.907311	11.376960
10.789404	784.624336	11.381978
11.137187	781.879946	11.386995
11.019277	786.380804	11.392013
10.612726	782.479111	11.397031
10.872914	781.523938	11.402048
10.841984	784.051833	11.407066
10.912845	781.302122	11.412083
11.158347	799.729876	11.417101
11.012391	800.475338	11.422119
11.310735	797.367498	11.427136
10.843576	800.292813	11.432154
11.262917	802.037917	11.437171
11.360822	801.213941	11.442189
11.180413	803.128829	11.447207
10.719085	791.797214	11.452224
10.732401	810.852377	11.457242
11.152927	820.210291	11.462259
11.306500	822.433637	11.467277
11.313710	814.378583	11.472295
12.087131	824.898080	11.477312
11.128791	810.208767	11.482330
11.535752	789.409038	11.487347
11.465991	799.737847	11.492365
11.172195	791.966102	11.497383
11.081570	784.629984	11.502400
11.029285	801.014248	11.507418
11.030723	786.554192	11.512435
10.794297	797.751500	11.517453
11.314479	808.258199	11.522471
11.450638	815.018845	11.527488
11.386332	823.620869	11.532506
11.431378	811.345586	11.537523
11.324038	815.938792	11.542541
11.172783	823.916270	11.547559
11.348013	811.824931	11.552576
11.420018	814.678681	11.557594
11.526075	820.639237	11.562611
11.345255	826.207165	11.567629
11.665099	820.346289	11.572647
11.522660	813.370689	11.577664
10.867436	809.878260	11.582682
11.391425	812.863059	11.587699
11.384867	815.462116	11.592717
11.309990	812.651498	11.597735
11.367467	819.974361	11.602752
11.357611	826.453695	11.607770
11.449554	824.456747	11.612787
11.374059	825.133852	11.617805
11.214472	819.421656	11.622823
11.401422	807.912996	11.627840
11.424101	821.392888	11.632858
11.322155	819.727246	11.637875
11.374341	822.308703	11.642893
11.404038	822.922721	11.647911
11.558961	818.954419	11.652928
11.310249	817.507559	11.657946
11.739701	819.882848	11.662963
11.602831	822.810951	11.667981
11.304536	813.561667	11.672999
11.871672	832.508612	11.678016
11.548608	836.228930	11.683034
11.602300	839.718364	11.688051
11.708416	847.981958	11.693069
11.518594	852.038073	11.698087
12.026687	843.865021	11.703104
11.584796	840.718736	11.708122
11.480150	831.500364	11.713139
11.628044	842.488400	11.718157
11.587114	850.598402	11.723175
11.785983	848.142033	11.728192
11.791728	853.630260	11.733210
11.463023	854.096553	11.738227
11.759397	857.961139	11.743245
11.773374	860.226110	11.748263
11.532517	851.183817	11.753280
11.526394	859.024293	11.758298
11.610016	849.380264	11.763315
12.032780	854.394729	11.768333
11.657616	865.926463	11.773351
11.557546	843.556370	11.778368
11.510413	866.965498	11.783386
11.424901	866.076226	11.788403
11.714148	856.178074	11.793421
11.450071	866.690673	11.798439
11.929613	859.833697	11.803456
11.854954	877.583887	11.808474
12.072518	874.232728	11.813491
12.368691	882.232202	11.818509
12.184359	866.486753	11.823527
12.170229	863.652681	11.828544
11.794906	867.291506	11.833562
11.718849	865.631020	11.838579
11.765793	852.074743	11.843597
11.626573	858.403473	11.848615
11.967699	865.747887	11.853632
12.162330	877.050241	11.858650
11.906457	873.694020	11.863667
12.170250	875.892823	11.868685
11.862426	870.714581	11.873703
11.921016	870.769118	11.878720
12.171755	881.901955	11.883738
12.349881	885.518425	11.888755
12.279608	869.671412	11.893773
11.849720	866.995159	11.898791
12.000213	866.549067	11.903808
12.175851	878.241163	11.908826
11.999396	876.715800	11.913843
12.416245	874.107982	11.918861
12.097392	876.549718	11.923879
12.120254	875.399204	11.928896
11.975856	869.000255	11.933914
12.018786	870.455352	11.938931
11.793529	879.400580	11.943949
11.952020	883.423432	11.948967
12.252394	867.194585	11.953984
12.028866	880.216109	11.959002
12.033826	887.531953	11.964019
12.118774	880.822985	11.969037
11.758394	887.176934	11.974055
12.034437	878.469089	11.979072
12.153111	886.206239	11.984090
12.193664	880.737637	11.989107
12.097120	888.588377	11.994125
12.334252	901.358447	11.999143
12.444729	906.843915	12.004160
12.066437	907.962487	12.009178
12.265947	914.742213	12.014195
12.306086	914.526196	12.019213
12.264253	914.277692	12.024231
12.477480	915.584520	12.029248
12.384794	907.381794	12.034266
12.609446	918.809122	12.039283
12.375442	916.126800	12.044301
12.293687	920.229207	12.049319
12.710228	906.129022	12.054336
12.373274	909.521751	12.059354
12.402982	914.106070	12.064371
12.439447	908.293663	12.069389
12.371278	908.874287	12.074407
12.334073	909.585604	12.079424
12.496677	909.131207	12.084442
12.595199	909.285821	12.089459
12.788072	908.579966	12.094477
12.520993	910.878888	12.099495
12.598061	906.062469	12.104512
12.604886	918.525431	12.109530
12.343007	904.334450	12.114547
12.439483	899.296326	12.119565
12.331764	915.944997	12.124583
12.549390	910.427378	12.129600
12.360573	905.942378	12.134618
12.174815	910.539149	12.139635
12.538377	905.262709	12.144653
12.434916	906.049169	12.149671
12.571912	910.585013	12.154688
12.757035	914.924709	12.159706
12.519218	914.829914	12.164723
12.906714	906.462243	12.169741
12.756425	909.147319	12.174759
12.917047	910.101849	12.179776
13.152086	904.356163	12.184794
12.786603	908.233515	12.189811
13.093947	904.091138	12.194829
12.568286	912.401121	12.199847
12.861760	898.654379	12.204864
12.465873	917.342021	12.209882
12.541704	915.196949	12.214899
12.921211	902.028057	12.219917
12.787353	913.787178	12.224935
12.649243	910.457902	12.229952
12.899397	906.530498	12.234970
12.731050	908.985504	12.239987
12.769992	911.699871	12.245005
12.807112	908.402994	12.250023
12.930317	903.852152	12.255040
12.946026	906.523124	12.260058
13.293290	916.534146	12.265075
13.233035	915.330073	12.270093
12.855891	911.677797	12.275111
13.133633	910.764589	12.280128
13.121823	905.851476	12.285146
13.038050	911.415174	12.290163
12.912500	910.585678	12.295181
12.884576	913.979987	12.300199
12.962091	909.921728	12.305216
13.183607	908.718632	12.310234
13.044224	914.812777	12.315251
13.355177	908.553752	12.320269
13.176244	912.216363	12.325287
13.182822	907.511219	12.330304
13.480360	912.167324	12.335322
12.994011	914.497832	12.340339
13.278604	911.815850	12.345357
13.120087	915.164859	12.350375
13.263013	918.212781	12.355392
12.986864	914.476460	12.360410
12.878639	918.974572	12.365427
13.237587	913.035536	12.370445
12.898056	911.241517	12.375463
13.125694	909.213821	12.380480
13.335059	902.659430	12.385498
13.229574	911.297847	12.390515
13.279003	903.864074	12.395533
12.804568	908.395661	12.400551
12.935460	903.521120	12.405568
13.189904	909.201243	12.410586
12.687649	907.882577	12.415603
12.823223	911.543893	12.420621
13.282679	933.212611	12.425639
13.038718	939.236685	12.430656
13.460218	930.862190	12.435674
13.234623	944.144335	12.440691
13.476471	932.229264	12.445709
13.232093	940.160807	12.450727
13.403147	941.576585	12.455744
13.469530	934.928540	12.460762
12.835450	944.838710	12.465779
13.467955	938.109908	12.470797
13.636087	943.633872	12.475815
13.406026	938.006134	12.480832
13.446864	934.976734	12.485850
13.505186	941.020434	12.490867
13.664942	944.404537	12.495885
13.437170	941.208994	12.500903
13.167166	945.226838	12.505920
13.684196	940.266690	12.510938
13.474487	943.511589	12.515955
13.579002	940.807456	12.520973
13.482260	944.172224	12.525991
13.484610	944.916362	12.531008
13.457007	929.484251	12.536026
13.513746	939.840628	12.541043
13.941067	932.216317	12.546061
13.631628	935.382064	12.551079
13.524574	943.207801	12.556096
13.695760	934.376349	12.561114
13.531151	939.140486	12.566131
13.408253	938.119612	12.571149
13.475959	934.570430	12.576167
13.477792	938.808993	12.581184
13.748690	938.857113	12.586202
13.166601	941.278673	12.591219
13.767174	940.192718	12.596237
13.845914	942.572562	12.601255
13.447146	940.262781	12.606272
13.757280	948.004082	12.611290
13.742874	970.628058	12.616307
14.074042	961.489795	12.621325
13.818032	948.450905	12.626343
13.627755	948.248635	12.631360
13.993795	947.196793	12.636378
13.522706	952.397889	12.641395
13.815780	958.396030	12.646413
13.998533	975.099809	12.651431
13.829556	970.215064	12.656448
14.090944	965.375585	12.661466
13.596304	976.277998	12.666483
13.770984	972.200484	12.671501
13.723331	968.965660	12.676519
14.002983	976.324638	12.681536
14.199923	973.127260	12.686554
13.862192	980.723116	12.691571
13.981873	981.194292	12.696589
14.221868	974.481655	12.701607
13.953302	983.016020	12.706624
14.429387	970.723957	12.711642
14.008598	970.361047	12.716659
13.981329	967.181114	12.721677
14.003000	960.977845	12.726695
13.912301	973.208191	12.731712
14.173749	964.131864	12.736730
13.929985	980.381890	12.741747
14.189545	966.670624	12.746765
14.358287	967.602554	12.751783
14.097015	973.858239	12.756800
14.064163	970.207202	12.761818
13.714757	964.233878	12.766835
13.737116	969.109576	12.771853
13.884083	972.574539	12.776871
14.005691	981.926935	12.781888
13.884424	970.619976	12.786906
14.000136	982.526790	12.791923
13.583468	965.715032	12.796941
13.951535	981.047240	12.801959
13.770666	992.427213	12.806976
14.144929	993.906192	12.811994
14.253482	1007.251950	12.817011
13.838401	1007.490434	12.822029
14.366950	1001.665794	12.827047
14.352173	1012.253345	12.832064
14.304926	998.197596	12.837082
13.990611	999.180388	12.842099
14.101452	1000.286469	12.847117
14.385830	996.020317	12.852135
14.456164	1000.769188	12.857152
14.583544	997.550648	12.862170
14.531401	998.248303	12.867187
14.460916	1001.539840	12.872205
14.552753	1000.979841	12.877223
14.406909	999.480104	12.882240
14.414715	996.901814	12.887258
14.509752	994.842524	12.892275
14.429406	992.821331	12.897293
14.295335	994.214021	12.902311
14.156970	1005.783414	12.907328
14.857453	1003.713231	12.912346
14.561862	1003.277621	12.917363
14.197136	997.550906	12.922381
14.798906	1002.470426	12.927399
14.511591	1008.633197	12.932416
14.642756	1002.390521	12.937434
14.556204	1016.629194	12.942451
14.673042	1020.769998	12.947469
14.881275	1016.571172	12.952487
14.830977	1013.995415	12.957504
14.263108	1001.245909	12.962522
14.889312	1019.860086	12.967539
14.486986	1019.110667	12.972557
14.907057	1022.634744	12.977575
14.474416	1021.728146	12.982592
14.611059	1029.990326	12.987610
14.809103	1024.962900	12.992627
14.448312	1025.234124	12.997645
14.907931	1026.248595	13.002663
14.567586	1026.640051	13.007680
14.764752	1026.928719	13.012698
14.717798	1028.218014	13.017715
14.818578	1025.431023	13.022733
14.898030	1019.715782	13.027751
15.164282	1031.909112	13.032768
15.243112	1021.394541	13.037786
15.326555	1026.058968	13.042803
14.952361	1015.058023	13.047821
15.003211	998.454234	13.052839
14.830532	997.423490	13.057856
15.136352	998.308315	13.062874
14.753583	1001.896044	13.067891
14.755063	1016.715785	13.072909
14.961089	1020.965045	13.077927
14.923394	1021.461890	13.082944
15.106636	1026.739689	13.087962
15.202858	1024.800667	13.092979
14.810407	1034.285856	13.097997
14.878004	1024.045575	13.103015
14.929650	1032.071446	13.108032
15.113608	1026.218823	13.113050
15.202147	1021.087489	13.118067
15.010078	1031.413084	13.123085
15.031950	1029.211973	13.128103
15.208984	1031.457842	13.133120
15.077629	1029.532489	13.138138
14.905640	1030.167317	13.143155
15.021028	1031.562007	13.148173
15.018834	1024.040272	13.153191
14.978271	1027.128836	13.158208
14.851309	1028.276267	13.163226
15.293758	1031.386813	13.168243
14.924104	1033.123231	13.173261
15.366905	1029.799699	13.178279
14.925119	1035.411309	13.183296
15.335022	1038.234343	13.188314
15.397831	1049.282677	13.193331
15.010791	1053.599446	13.198349
15.628941	1043.116021	13.203367
15.454585	1055.788222	13.208384
15.539361	1037.700084	13.213402
15.349159	1035.787231	13.218419
15.378293	1034.543544	13.223437
15.577284	1029.676584	13.228455
15.502836	1026.373354	13.233472
15.431290	1027.443107	13.238490
15.469485	1021.880755	13.243507
15.087739	1030.457116	13.248525
15.639465	1022.692873	13.253543
15.727986	1029.233164	13.258560
15.406005	1027.950773	13.263578
15.734172	1021.452247	13.268595
15.346200	1033.718876	13.273613
15.404825	1024.313121	13.278631
15.656244	1031.711838	13.283648
15.686922	1038.016838	13.288666
15.836186	1028.115380	13.293683
15.029416	1029.344282	13.298701
15.489842	1040.940918	13.303719
15.509540	1053.516813	13.308736
15.581461	1053.470722	13.313754
15.919668	1056.798921	13.318771
15.643362	1058.716335	13.323789
15.707773	1051.070569	13.328807
15.757125	1055.396962	13.333824
15.560481	1061.968740	13.338842
15.995024	1059.198125	13.343859
15.504771	1060.255329	13.348877
15.712260	1055.749933	13.353895
15.502297	1060.014154	13.358912
15.416011	1056.784922	13.363930
15.895553	1060.949138	13.368947
15.632413	1063.492697	13.373965
15.603453	1057.452493	13.378983
15.914647	1047.326971	13.384000
15.664512	1056.798843	13.389018
15.565939	1058.151016	13.394035
15.468130	1060.898291	13.399053
15.722751	1069.666135	13.404071
16.039745	1089.187083	13.409088
15.864997	1089.373958	13.414106
16.016402	1082.449574	13.419123
16.469433	1088.030346	13.424141
15.811812	1068.523426	13.429159
16.028173	1073.223336	13.434176
15.869871	1087.885358	13.439194
16.120076	1083.408707	13.444211
15.752270	1091.114317	13.449229
16.192328	1090.674204	13.454247
16.193765	1092.642083	13.459264
15.700823	1099.207432	13.464282
16.189592	1088.915080	13.469299
15.854572	1096.862500	13.474317
16.057148	1078.431589	13.479335
15.729373	1090.712703	13.484352
16.049037	1083.701009	13.489370
16.144225	1091.144129	13.494387
15.880551	1097.366404	13.499405
16.112740	1079.837252	13.504423
16.286999	1081.983197	13.509440
16.251956	1089.625041	13.514458
16.252044	1081.835586	13.519475
15.806423	1084.481411	13.524493
15.985124	1084.840459	13.529511
15.987152	1095.322925	13.534528
16.221804	1110.903725	13.539546
16.374645	1107.704175	13.544563
16.236685	1116.423278	13.549581
16.413671	1116.350340	13.554599
16.609334	1111.743346	13.559616
16.412729	1117.616345	13.564634
16.549039	1101.984877	13.569651
16.495726	1111.313563	13.574669
16.456355	1110.680408	13.579687
16.597685	1110.569282	13.584704
16.596567	1103.170949	13.589722
16.629699	1106.078433	13.594739
16.125524	1101.592055	13.599757
16.137856	1106.191119	13.604775
16.509474	1108.815394	13.609792
16.294182	1109.510937	13.614810
16.633674	1097.976409	13.619827
16.622750	1114.206914	13.624845
16.659153	1106.575995	13.629863
16.615368	1105.455004	13.634880
16.483811	1111.490058	13.639898
16.852784	1111.106597	13.644915
16.684063	1113.324695	13.649933
16.612427	1106.876198	13.654951
16.482606	1104.858852	13.659968
16.615013	1110.611226	13.664986
16.682757	1103.816824	13.670003
16.636185	1112.339695	13.675021
16.864651	1108.587874	13.680039
17.145379	1109.059944	13.685056
17.226257	1116.973148	13.690074
17.648900	1104.331573	13.695091
16.656873	1095.820994	13.700109
16.621658	1096.865050	13.705127
17.081486	1112.884141	13.710144
16.998168	1108.983561	13.715162
16.862116	1077.333160	13.720179
16.934337	1091.346010	13.725197
16.812566	1077.767868	13.730215
17.351391	1088.285451	13.735232
17.001887	1082.292019	13.740250
16.952671	1077.277963	13.745267
16.905420	1077.420498	13.750285
16.692854	1079.407671	13.755303
17.079007	1091.589461	13.760320
16.863270	1091.841390	13.765338
17.007056	1112.089845	13.770355
17.045653	1109.269044	13.775373
17.020183	1109.104832	13.780391
17.048683	1113.765393	13.785408
16.840302	1117.066404	13.790426
16.972253	1110.751904	13.795443
16.819802	1108.732400	13.800461
16.504747	1117.687910	13.805479
16.836500	1107.991214	13.810496
16.953237	1120.262520	13.815514
16.815247	1113.077786	13.820531
16.902763	1124.968907	13.825549
17.306531	1129.120099	13.830567
17.545776	1137.266530	13.835584
17.171312	1139.267529	13.840602
17.180341	1141.533360	13.845619
17.246134	1137.376592	13.850637
17.138082	1138.896480	13.855655
17.571125	1145.901407	13.860672
17.164953	1146.184872	13.865690
17.420891	1138.925839	13.870707
17.155625	1155.053233	13.875725
17.459303	1151.055489	13.880743
17.614268	1142.247078	13.885760
17.556157	1147.042066	13.890778
17.591667	1145.230008	13.895795
17.445319	1146.721199	13.900813
17.543951	1150.062320	13.905831
17.571793	1145.036663	13.910848
17.384426	1127.341507	13.915866
17.386194	1140.610184	13.920883
17.528381	1135.691576	13.925901
17.390397	1139.183685	13.930919
17.578587	1141.754091	13.935936
17.305911	1144.866548	13.940954
17.575273	1138.798171	13.945971
17.762602	1143.790697	13.950989
17.883406	1141.608226	13.956007
17.739855	1136.468438	13.961024
17.624393	1138.211593	13.966042
17.559768	1142.031308	13.971059
17.481438	1149.073675	13.976077
17.459394	1137.019475	13.981095
17.763615	1133.636194	13.986112
17.622661	1130.463637	13.991130
17.708368	1132.016396	13.996147
17.517351	1139.946684	14.001165
17.427903	1139.594254	14.006183
17.970044	1131.213453	14.011200
17.693091	1139.371351	14.016218
17.717903	1140.051150	14.021235
17.879583	1142.440125	14.026253
17.730604	1137.072501	14.031271
17.736619	1138.961677	14.036288
17.800896	1146.352858	14.041306
17.649996	1157.611062	14.046323
18.261137	1165.416405	14.051341
18.157050	1166.828948	14.056359
18.234109	1157.404312	14.061376
17.923872	1156.024299	14.066394
18.217578	1143.694192	14.071411
18.239419	1143.772926	14.076429
17.923402	1139.350259	14.081447
18.247823	1135.343966	14.086464
18.087139	1138.779993	14.091482
18.269851	1136.255391	14.096499
18.179655	1134.482654	14.101517
17.828379	1141.855640	14.106535
18.024032	1138.383253	14.111552
17.577081	1149.576700	14.116570
17.998130	1157.052503	14.121587
18.169116	1160.332040	14.126605
18.136098	1171.445541	14.131623
18.183195	1167.546578	14.136640
18.044091	1170.182210	14.141658
18.318883	1161.630316	14.146675
18.313973	1169.866012	14.151693
18.054613	1178.158415	14.156711
18.268299	1165.704537	14.161728
18.236405	1169.212155	14.166746
18.229127	1167.160730	14.171763
18.209034	1168.418029	14.176781
18.256718	1169.531039	14.181799
18.237560	1167.935505	14.186816
18.002469	1166.410768	14.191834
18.067706	1176.173786	14.196851
18.637095	1181.534148	14.201869
18.631934	1201.155433	14.206887
18.896649	1191.445771	14.211904
18.792068	1168.885804	14.216922
18.840789	1159.974507	14.221939
18.624724	1151.471225	14.226957
18.463101	1158.880922	14.231975
18.433764	1147.510186	14.236992
18.658674	1152.497672	14.242010
18.832760	1153.952337	14.247027
18.668935	1149.547770	14.252045
18.337103	1152.499164	14.257063
18.420774	1150.918887	14.262080
18.489749	1145.609261	14.267098
18.546947	1158.621538	14.272115
18.692157	1170.655104	14.277133
18.802171	1188.170350	14.282151
19.061411	1170.330325	14.287168
18.892467	1164.750256	14.292186
18.805921	1161.752142	14.297203
18.812607	1146.357836	14.302221
18.908254	1149.439223	14.307239
18.925602	1141.653573	14.312256
18.860368	1148.150085	14.317274
18.903136	1143.793197	14.322291
19.273370	1149.960127	14.327309
19.008863	1148.027675	14.332327
19.235517	1146.227664	14.337344
18.967436	1145.404435	14.342362
19.148736	1152.835294	14.347379
19.169440	1137.253248	14.352397
18.971611	1145.773627	14.357415
18.962243	1129.823351	14.362432
19.005690	1132.731494	14.367450
19.037634	1146.848304	14.372467
19.088877	1142.410882	14.377485
18.947689	1154.103290	14.382503
19.205975	1139.782257	14.387520
19.162500	1141.857970	14.392538
18.987675	1147.102588	14.397555
18.841752	1133.913031	14.402573
18.606328	1151.710628	14.407591
18.730677	1160.743790	14.412608
19.076517	1170.696946	14.417626
19.274181	1174.226786	14.422643
19.695338	1176.920427	14.427661
19.255050	1185.667586	14.432679
19.558241	1177.629471	14.437696
19.323232	1175.816931	14.442714
19.344058	1183.653895	14.447731
19.735713	1179.215209	14.452749
19.390878	1187.032413	14.457767
19.186196	1182.013753	14.462784
19.014723	1188.238906	14.467802
19.421154	1182.463161	14.472819
19.396969	1179.712977	14.477837
19.349313	1187.006968	14.482855
19.348008	1178.777155	14.487872
19.409125	1177.081322	14.492890
19.146451	1181.939722	14.497907
19.530483	1179.640824	14.502925
19.257633	1182.374981	14.507943
19.201416	1180.790307	14.512960
19.419151	1182.777103	14.517978
19.411360	1185.808698	14.522995
19.429505	1176.176490	14.528013
19.296664	1210.309494	14.533031
19.649160	1208.426435	14.538048
19.656059	1204.031770	14.543066
19.675836	1220.316750	14.548083
20.222767	1203.892004	14.553101
19.664542	1215.417696	14.558119
19.876137	1208.843910	14.563136
19.636753	1208.239148	14.568154
19.825332	1208.628845	14.573171
19.814836	1205.551202	14.578189
20.310069	1211.798242	14.583207
20.245033	1192.476494	14.588224
20.052975	1184.276691	14.593242
19.594352	1178.060746	14.598259
19.773677	1171.738769	14.603277
19.802064	1180.240210	14.608295
19.884000	1183.841577	14.613312
19.957637	1188.375397	14.618330
20.085664	1197.259550	14.623347
20.148987	1199.079009	14.628365
20.026786	1182.959572	14.633383
19.862376	1184.224236	14.638400
20.121530	1190.598941	14.643418
20.261524	1205.273882	14.648435
20.409813	1184.574726	14.653453
20.294059	1184.683725	14.658471
20.059767	1178.914084	14.663488
20.139388	1173.422375	14.668506
19.666068	1165.870715	14.673523
20.110548	1175.012680	14.678541
20.597685	1199.907419	14.683559
19.906714	1188.004105	14.688576
20.481787	1178.701314	14.693594
20.151018	1199.334758	14.698611
20.614363	1199.831709	14.703629
20.254691	1187.224339	14.708647
20.125193	1183.277846	14.713664
20.611816	1182.156023	14.718682
20.348316	1180.769055	14.723699
20.354773	1174.652470	14.728717
20.042248	1180.721455	14.733735
20.297090	1196.499387	14.738752
20.374911	1205.698543	14.743770
20.415496	1200.662884	14.748787
20.384016	1202.426784	14.753805
20.354695	1195.177167	14.758823
20.745297	1200.950597	14.763840
20.551973	1191.796693	14.768858
20.694059	1205.536666	14.773875
20.373527	1206.351605	14.778893
20.342247	1200.157403	14.783911
20.265689	1202.917719	14.788928
20.658560	1197.119018	14.793946
20.529728	1202.209585	14.798963
20.497013	1199.624192	14.803981
20.708053	1203.303395	14.808999
20.432465	1194.554440	14.814016
20.693089	1200.616316	14.819034
20.365741	1203.944526	14.824051
20.723107	1209.995109	14.829069
20.927312	1235.194624	14.834087
20.696893	1236.952889	14.839104
21.213773	1233.530041	14.844122
20.610203	1220.455170	14.849139
21.039327	1216.663796	14.854157
20.409080	1211.475446	14.859175
20.695786	1227.459939	14.864192
20.765829	1228.507834	14.869210
20.854275	1236.758814	14.874227
20.874814	1234.185857	14.879245
20.915633	1239.003466	14.884263
20.895977	1235.770250	14.889280
20.949157	1225.527105	14.894298
21.167479	1232.208976	14.899315
20.857371	1229.509674	14.904333
21.237686	1234.602158	14.909351
21.084504	1235.598438	14.914368
21.214838	1228.868025	14.919386
20.854847	1237.954664	14.924403
21.307723	1229.596073	14.929421
20.942166	1228.295290	14.934439
20.833189	1228.502772	14.939456
20.814312	1232.860590	14.944474
20.830328	1229.166361	14.949491
21.182152	1246.486516	14.954509
21.672748	1250.036762	14.959527
21.344097	1252.145540	14.964544
21.508475	1242.955206	14.969562
21.368967	1246.359405	14.974579
21.528154	1239.611611	14.979597
21.626579	1217.592746	14.984615
21.428244	1230.702908	14.989632
21.298943	1221.991524	14.994650
21.285509	1224.162270	14.999667
21.575679	1215.922359	15.004685
21.256570	1224.786478	15.009703
21.664979	1246.005045	15.014720
21.642614	1247.834368	15.019738
21.572456	1240.577714	15.024755
21.666666	1225.105453	15.029773
21.822133	1217.774440	15.034791
21.441861	1224.094418	15.039808
21.983034	1206.356087	15.044826
21.655145	1216.719256	15.049843
21.645146	1210.496329	15.054861
21.910929	1215.922727	15.059879
21.649999	1220.207241	15.064896
21.630416	1211.121403	15.069914
21.536033	1227.332777	15.074931
21.610487	1220.262811	15.079949
21.878967	1228.937114	15.084967
21.751009	1247.375277	15.089984
22.086731	1242.365927	15.095002
21.664821	1242.875616	15.100019
22.029928	1244.538416	15.105037
21.955212	1243.071757	15.110055
21.797518	1243.726666	15.115072
22.082297	1248.599941	15.120090
22.170181	1254.514856	15.125107
22.197200	1233.830992	15.130125
22.014809	1222.783570	15.135143
21.409413	1232.724997	15.140160
21.783937	1233.198075	15.145178
21.834365	1242.434466	15.150195
21.652807	1240.970933	15.155213
22.228662	1241.017374	15.160231
21.976977	1254.259617	15.165248
22.187562	1244.278577	15.170266
21.970890	1256.463866	15.175283
22.061993	1246.176633	15.180301
22.090491	1242.868120	15.185319
21.753606	1249.637213	15.190336
21.917339	1243.977617	15.195354
22.267008	1265.363808	15.200371
22.125291	1276.259955	15.205389
22.595357	1272.642100	15.210407
22.283981	1273.614578	15.215424
22.375268	1276.605769	15.220442
22.771248	1280.776797	15.225459
22.256065	1265.510523	15.230477
22.973641	1249.076369	15.235495
22.084736	1250.458647	15.240512
22.301175	1241.176231	15.245530
22.347688	1247.414916	15.250547
22.296651	1258.075961	15.255565
22.580159	1259.135359	15.260583
22.590053	1271.734313	15.265600
22.405331	1272.191735	15.270618
22.458695	1272.994762	15.275635
22.463261	1270.859474	15.280653
22.925615	1270.635346	15.285671
22.754185	1274.397979	15.290688
23.010743	1271.315075	15.295706
22.919663	1265.454758	15.300723
22.861494	1271.771416	15.305741
22.892421	1262.231918	15.310759
22.652919	1259.087069	15.315776
22.810261	1256.730819	15.320794
22.744891	1276.030286	15.325811
22.572220	1271.306684	15.330829
22.741803	1263.004435	15.335847
22.958519	1267.657102	15.340864
22.774449	1270.315551	15.345882
22.897912	1266.661393	15.350899
22.756465	1267.418728	15.355917
22.950550	1269.679131	15.360935
22.927075	1272.870030	15.365952
23.148225	1271.761454	15.370970
23.108772	1269.337004	15.375987
22.871231	1275.501480	15.381005
22.941532	1266.749931	15.386023
23.077947	1269.787190	15.391040
22.897657	1265.442796	15.396058
23.089067	1265.535970	15.401075
23.095982	1266.061261	15.406093
23.215146	1262.860957	15.411111
22.858708	1270.384854	15.416128
22.846516	1260.786357	15.421146
23.308158	1274.401035	15.426163
23.405950	1287.473627	15.431181
23.741984	1279.124909	15.436199
23.622004	1276.382697	15.441216
23.202031	1261.990012	15.446234
23.148107	1263.468271	15.451251
23.199161	1267.452323	15.456269
23.386638	1255.005076	15.461287
23.328589	1267.836927	15.466304
23.464907	1283.781028	15.471322
23.430469	1283.007682	15.476339
23.372219	1287.851554	15.481357
23.767153	1283.083956	15.486375
23.522878	1288.762948	15.491392
23.763977	1290.604159	15.496410
23.624581	1285.064428	15.501427
23.589364	1287.704923	15.506445
23.665676	1273.673345	15.511463
23.607732	1286.346536	15.516480
23.660590	1286.799654	15.521498
23.657553	1280.235396	15.526515
23.513361	1285.310424	15.531533
23.641265	1283.541316	15.536551
23.695998	1289.925505	15.541568
23.609278	1291.653287	15.546586
23.604995	1280.916481	15.551603
23.641746	1290.303194	15.556621
23.729939	1279.483754	15.561639
23.645882	1288.181429	15.566656
23.667882	1288.817214	15.571674
23.911112	1279.935055	15.576691
23.498908	1285.188712	15.581709
23.578109	1289.427946	15.586727
23.667381	1302.649989	15.591744
24.073058	1312.228375	15.596762
24.302015	1315.243233	15.601779
24.294550	1327.189607	15.606797
24.439173	1299.451262	15.611815
23.959065	1297.380875	15.616832
24.042080	1293.767660	15.621850
23.979902	1305.998663	15.626867
23.881820	1316.329355	15.631885
23.953358	1318.940761	15.636903
24.255821	1316.643934	15.641920
24.100319	1317.323679	15.646938
24.088168	1312.606553	15.651955
23.921178	1316.339327	15.656973
24.283285	1316.812496	15.661991
24.448529	1310.620352	15.667008
24.487847	1311.174137	15.672026
24.517220	1316.908217	15.677043
24.221853	1315.788320	15.682061
24.276637	1309.814070	15.687079
24.447313	1312.457089	15.692096
24.501589	1316.344952	15.697114
24.560272	1318.817150	15.702131
24.485402	1318.538677	15.707149
24.398498	1311.613497	15.712167
24.320522	1320.188532	15.717184
24.234661	1318.222933	15.722202
24.695046	1325.613172	15.727219
24.463788	1340.915063	15.732237
24.811301	1331.605377	15.737255
24.880566	1333.834097	15.742272
24.704134	1332.573640	15.747290
24.892082	1337.914545	15.752307
24.846055	1329.501510	15.757325
24.863327	1325.659021	15.762343
24.892662	1322.360195	15.767360
24.866782	1327.598712	15.772378
24.891916	1324.763172	15.777395
24.675385	1320.940896	15.782413
24.941006	1321.195795	15.787431
24.826935	1327.681966	15.792448
24.885619	1327.441613	15.797466
25.126472	1322.800303	15.802483
25.294919	1332.490425	15.807501
25.293342	1323.394846	15.812519
25.151596	1311.684343	15.817536
24.714074	1301.705865	15.822554
25.273728	1312.280388	15.827571
24.905623	1326.948638	15.832589
25.441421	1326.619831	15.837607
25.213195	1324.407731	15.842624
25.174092	1328.310666	15.847642
25.577280	1322.525959	15.852659
25.205444	1306.164271	15.857677
24.811836	1297.750543	15.862695
25.085224	1307.291778	15.867712
25.082111	1311.049382	15.872730
25.439495	1314.057933	15.877747
25.142978	1326.959242	15.882765
25.261332	1317.012326	15.887783
25.431920	1328.721347	15.892800
25.358429	1324.440352	15.897818
25.158207	1319.670116	15.902835
25.339845	1326.279364	15.907853
25.403713	1327.436160	15.912871
25.233035	1326.386952	15.917888
25.220159	1327.074181	15.922906
25.514706	1327.205001	15.927923
25.307387	1326.967752	15.932941
25.516742	1342.139596	15.937959
25.824060	1349.236695	15.942976
25.505335	1357.667368	15.947994
25.935965	1353.048560	15.953011
25.798312	1356.826091	15.958029
26.104305	1345.037089	15.963047
25.545462	1324.774916	15.968064
25.733397	1340.184947	15.973082
26.023103	1328.512432	15.978099
26.093716	1336.992793	15.983117
25.918465	1333.143994	15.988135
26.007399	1312.908819	15.993152
25.757078	1314.346772	15.998170
26.149154	1314.237036	16.003187
26.054734	1318.697150	16.008205
25.782934	1313.763969	16.013223
26.221919	1318.179456	16.018240
26.193547	1315.231914	16.023258
26.141137	1306.441214	16.028275
25.841098	1311.438910	16.033293
26.025343	1319.840604	16.038311
26.213078	1341.137182	16.043328
25.967825	1351.962339	16.048346
26.246639	1343.077008	16.053363
26.403686	1346.915184	16.058381
26.207764	1343.762314	16.063399
26.244575	1345.722398	16.068416
26.218427	1353.281799	16.073434
26.189446	1354.446886	16.078451
26.255402	1354.991931	16.083469
26.204727	1346.284778	16.088487
26.246682	1349.861309	16.093504
26.160517	1348.194571	16.098522
26.333253	1343.412962	16.103539
26.297578	1336.858021	16.108557
26.617986	1347.887928	16.113575
26.793835	1339.028310	16.118592
26.179960	1346.321256	16.123610
26.621238	1343.434912	16.128627
26.496176	1344.562366	16.133645
26.734098	1338.144794	16.138663
26.669187	1341.914213	16.143680
26.392769	1347.006826	16.148698
26.401964	1337.062225	16.153715
26.731631	1355.116474	16.158733
26.559172	1370.160235	16.163751
26.853271	1371.451743	16.168768
26.531372	1375.756238	16.173786
26.988353	1367.899643	16.178803
26.948385	1375.344415	16.183821
26.697443	1374.532507	16.188839
27.169185	1366.321111	16.193856
27.170128	1371.111113	16.198874
27.060319	1370.020327	16.203891
26.841453	1375.472705	16.208909
26.908660	1373.165221	16.213927
27.296511	1367.817282	16.218944
26.899874	1383.125340	16.223962
27.341788	1371.942542	16.228979
27.220721	1372.119744	16.233997
27.062450	1381.774629	16.239015
26.972243	1368.208723	16.244032
27.013597	1378.597468	16.249050
27.212187	1380.259512	16.254067
27.184909	1375.336213	16.259085
27.012496	1376.754184	16.264103
27.321359	1372.422459	16.269120
26.941900	1378.769529	16.274138
27.296166	1371.196866	16.279155
27.044454	1366.606006	16.284173
27.189446	1376.907905	16.289191
27.592039	1374.105520	16.294208
27.284215	1366.651157	16.299226
27.274884	1367.072845	16.304243
27.155745	1373.259484	16.309261
27.181346	1383.432341	16.314279
27.594721	1381.200996	16.319296
27.694084	1403.379998	16.324314
27.457079	1406.649590	16.329331
27.912928	1410.399720	16.334349
27.720492	1405.471084	16.339367
27.841454	1397.317364	16.344384
27.726876	1407.597306	16.349402
27.790404	1403.210530	16.354419
27.679335	1400.678629	16.359437
27.920688	1399.113948	16.364455
27.929581	1393.452774	16.369472
27.762552	1397.079669	16.374490
27.829835	1397.368987	16.379507
28.074530	1384.998774	16.384525
27.834125	1395.651508	16.389543
28.375194	1376.823252	16.394560
28.047429	1388.257365	16.399578
28.007124	1394.140412	16.404595
28.253398	1391.180052	16.409613
28.048347	1395.794727	16.414631
28.345120	1393.356708	16.419648
28.186705	1392.223969	16.424666
28.445346	1382.807316	16.429683
28.339470	1366.027908	16.434701
28.240287	1363.828292	16.439719
28.191700	1355.464090	16.444736
28.022727	1365.703407	16.449754
27.982008	1376.997461	16.454771
28.080388	1388.067312	16.459789
27.868328	1390.222548	16.464807
27.929341	1382.309863	16.469824
27.695939	1392.877971	16.474842
28.114817	1392.039003	16.479859
28.428759	1407.447920	16.484877
28.572067	1421.580005	16.489895
28.354290	1407.037168	16.494912
28.732087	1412.781303	16.499930
28.608387	1412.001472	16.504947
28.746818	1403.218879	16.509965
28.489617	1409.971302	16.514983
28.888963	1405.235613	16.520000
28.801175	1411.608413	16.525018
28.923057	1400.306150	16.530035
28.765991	1388.994970	16.535053
28.690479	1387.453627	16.540071
28.684123	1383.048114	16.545088
28.657471	1391.051311	16.550106
28.895618	1408.381811	16.555123
29.134780	1406.630487	16.560141
28.952591	1392.712472	16.565159
28.943521	1379.817756	16.570176
28.986103	1380.531237	16.575194
28.984244	1390.524790	16.580211
28.859141	1366.351023	16.585229
28.736422	1397.737529	16.590247
28.857916	1397.232841	16.595264
28.728429	1403.147587	16.600282
28.841305	1409.480071	16.605299
29.254509	1401.929917	16.610317
29.028743	1414.961314	16.615335
29.121498	1400.104860	16.620352
29.079878	1413.082928	16.625370
29.020455	1411.247189	16.630387
29.265401	1403.124116	16.635405
29.185488	1410.325129	16.640423
29.324751	1409.214355	16.645440
29.274159	1406.918105	16.650458
29.349552	1407.839144	16.655475
29.413792	1400.779054	16.660493
29.086385	1413.102486	16.665511
29.467612	1426.092433	16.670528
29.539530	1433.235638	16.675546
29.779709	1442.226162	16.680563
29.882560	1438.549000	16.685581
29.609133	1423.470092	16.690599
29.690335	1419.259911	16.695616
29.521473	1410.028992	16.700634
29.280176	1426.337736	16.705651
29.544903	1429.712043	16.710669
29.263287	1447.299125	16.715687
29.407251	1444.168692	16.720704
29.617810	1432.165508	16.725722
29.608622	1433.166695	16.730739
29.651762	1436.225732	16.735757
29.940678	1442.825533	16.740775
30.055321	1433.561828	16.745792
29.848543	1435.047304	16.750810
29.594064	1432.889536	16.755827
29.741593	1437.276943	16.760845
29.734247	1456.541043	16.765863
30.247442	1452.522702	16.770880
30.561337	1453.016458	16.775898
30.109601	1457.534599	16.780915
30.633741	1459.583291	16.785933
30.437970	1448.219028	16.790951
30.512416	1435.105714	16.795968
30.646220	1425.041211	16.800986
30.258853	1433.469905	16.806003
30.262619	1421.064364	16.811021
30.054810	1423.473622	16.816039
30.317350	1420.434974	16.821056
30.492234	1419.423024	16.826074
30.148056	1423.660356	16.831091
30.449020	1425.883006	16.836109
30.477396	1428.822834	16.841127
30.631014	1426.697488	16.846144
30.425348	1428.411123	16.851162
30.676876	1425.630595	16.856179
30.363305	1412.521317	16.861197
30.238910	1431.454772	16.866215
30.593526	1446.329833	16.871232
30.601976	1446.444644	16.876250
30.489453	1449.461350	16.881267
30.508200	1448.170926	16.886285
30.781549	1449.330445	16.891303
31.036037	1446.371865	16.896320
30.974817	1444.228155	16.901338
30.778776	1446.192559	16.906355
30.901599	1449.256514	16.911373
30.840398	1453.145029	16.916391
30.754935	1447.541585	16.921408
30.788614	1446.592779	16.926426
30.560821	1440.044018	16.931443
30.822881	1436.936155	16.936461
30.771359	1441.312824	16.941479
30.843617	1449.696126	16.946496
31.162993	1451.775968	16.951514
31.276495	1470.720077	16.956531
31.361789	1465.254097	16.961549
31.029270	1458.363617	16.966567
31.335014	1459.885486	16.971584
31.087750	1466.249283	16.976602
31.257236	1489.686078	16.981619
31.633985	1472.465221	16.986637
31.651320	1478.896231	16.991655
31.285116	1451.107952	16.996672
31.510146	1451.634927	17.001690
31.180090	1454.727420	17.006707
31.734585	1463.741499	17.011725
31.583519	1467.578364	17.016743
31.742237	1462.192746	17.021760
31.798822	1447.752075	17.026778
31.357142	1441.973762	17.031795
31.502760	1449.897283	17.036813
31.532371	1463.566348	17.041831
31.151427	1468.002691	17.046848
31.637360	1464.464842	17.051866
31.532005	1483.257414	17.056883
31.623497	1465.689314	17.061901
31.427982	1475.786643	17.066919
31.601855	1469.769383	17.071936
31.670351	1463.597529	17.076954
31.617979	1475.799484	17.081971
32.060599	1482.067159	17.086989
31.933399	1498.708657	17.092007
32.047833	1497.578761	17.097024
32.441498	1500.505358	17.102042
32.142841	1487.283705	17.107059
32.319676	1467.209362	17.112077
31.893338	1471.995741	17.117095
32.131626	1464.557198	17.122112
32.483205	1463.305358	17.127130
32.035049	1470.844539	17.132147
32.274599	1465.323095	17.137165
32.288021	1483.263722	17.142183
32.086935	1486.329352	17.147200
32.189778	1480.593140	17.152218
32.280580	1489.910000	17.157235
32.349056	1480.898398	17.162253
32.434673	1487.385033	17.167271
32.561865	1496.113986	17.172288
32.591092	1476.550685	17.177306
32.323946	1492.780314	17.182323
32.649425	1486.894636	17.187341
32.503702	1488.376700	17.192359
32.232009	1485.497369	17.197376
32.535579	1486.648737	17.202394
32.587536	1483.207549	17.207411
32.487996	1481.225691	17.212429
32.540167	1481.129327	17.217447
32.449487	1488.690817	17.222464
32.736103	1495.752043	17.227482
32.592685	1510.489164	17.232499
33.059757	1515.917769	17.237517
33.091471	1525.125538	17.242535
33.182063	1512.111454	17.247552
33.300996	1495.873416	17.252570
33.092150	1494.585635	17.257587
33.273119	1482.923137	17.262605
33.097704	1486.167192	17.267623
33.136686	1479.258098	17.272640
33.361271	1472.647799	17.277658
33.246145	1476.575565	17.282675
33.231161	1470.089188	17.287693
33.078250	1471.616535	17.292711
33.112036	1476.088535	17.297728
33.419125	1469.039382	17.302746
33.013430	1481.143943	17.307763
33.063177	1478.977916	17.312781
33.522936	1489.905717	17.317799
33.192139	1506.716369	17.322816
33.620151	1500.990084	17.327834
33.241169	1502.764711	17.332851
33.614604	1504.925372	17.337869
33.433917	1506.589211	17.342887
33.522874	1515.512299	17.347904
33.519041	1498.191049	17.352922
33.906464	1500.373016	17.357939
33.720886	1500.673498	17.362957
34.050038	1505.654469	17.367975
33.740467	1502.105033	17.372992
33.703347	1496.300653	17.378010
33.834591	1499.212043	17.383027
33.944084	1496.318802	17.388045
34.060811	1493.950345	17.393063
33.887811	1498.161713	17.398080
33.886983	1491.918257	17.403098
33.896198	1501.560050	17.408115
33.775377	1503.589958	17.413133
34.139107	1504.986876	17.418151
33.778177	1503.014440	17.423168
33.972254	1498.287911	17.428186
33.739644	1499.987512	17.433203
33.705407	1503.692837	17.438221
34.106096	1502.203336	17.443239
33.902806	1525.990889	17.448256
34.204727	1515.609120	17.453274
34.295402	1531.339382	17.458291
34.370132	1536.778633	17.463309
34.427293	1530.717684	17.468327
34.565945	1537.078236	17.473344
34.604860	1526.282926	17.478362
34.557484	1531.552631	17.483379
34.437988	1524.556374	17.488397
34.576399	1528.411067	17.493415
34.769481	1527.107122	17.498432
34.899679	1523.628166	17.503450
34.615668	1526.806748	17.508467
34.382271	1523.318315	17.513485
34.969841	1525.937220	17.518503
34.841619	1529.290398	17.523520
34.757177	1528.835554	17.528538
34.863569	1526.974707	17.533555
34.766560	1520.995590	17.538573
34.702046	1516.663055	17.543591
34.797476	1530.454744	17.548608
34.684388	1527.147175	17.553626
35.073485	1524.404085	17.558643
34.560953	1527.393737	17.563661
34.951210	1520.659527	17.568679
34.647123	1523.791433	17.573696
34.517146	1525.339003	17.578714
34.841448	1538.468000	17.583731
34.895726	1547.779919	17.588749
34.994720	1550.587999	17.593767
35.053781	1553.610958	17.598784
35.201707	1547.516076	17.603802
35.398551	1552.315033	17.608819
34.996876	1555.610349	17.613837
35.623182	1536.706368	17.618855
35.404034	1547.513953	17.623872
35.387740	1547.637193	17.628890
35.671070	1542.458865	17.633907
35.662852	1551.559483	17.638925
35.558942	1545.350397	17.643943
35.736740	1542.961583	17.648960
35.301298	1536.647952	17.653978
35.605510	1542.098416	17.658995
35.843457	1539.969327	17.664013
36.093524	1537.818546	17.669031
35.745924	1548.658820	17.674048
36.021609	1550.599060	17.679066
36.120340	1541.844617	17.684083
35.726915	1547.790919	17.689101
36.119869	1540.482240	17.694119
35.974810	1547.334656	17.699136
36.058575	1545.305112	17.704154
35.772708	1537.257662	17.709171
35.790622	1551.742912	17.714189
36.146971	1541.202507	17.719207
36.147300	1542.297794	17.724224
36.237648	1542.575422	17.729242
36.408160	1543.253160	17.734259
36.232193	1536.324123	17.739277
36.358817	1541.452814	17.744295
36.085545	1551.802437	17.749312
36.338941	1541.738133	17.754330
36.276267	1540.040713	17.759347
35.988529	1532.114440	17.764365
36.610981	1555.421212	17.769383
36.526281	1568.911267	17.774400
36.468359	1565.914633	17.779418
36.915757	1565.120540	17.784435
36.707346	1549.929168	17.789453
36.831337	1534.642611	17.794471
36.725896	1532.986131	17.799488
36.549722	1531.473253	17.804506
36.630614	1534.754797	17.809523
36.310194	1549.232290	17.814541
36.797734	1557.797671	17.819559
36.913157	1568.093570	17.824576
36.635666	1563.941171	17.829594
36.648289	1569.058040	17.834611
36.717007	1561.277058	17.839629
37.048698	1567.045422	17.844647
36.812620	1570.165682	17.849664
36.898784	1561.153072	17.854682
37.004813	1557.930473	17.859699
36.470343	1564.324545	17.864717
37.117958	1574.866969	17.869735
37.086829	1588.376123	17.874752
37.228477	1605.992115	17.879770
37.410381	1601.212847	17.884787
37.447250	1605.002484	17.889805
37.671144	1587.963110	17.894823
37.212392	1582.348594	17.899840
37.052625	1579.264491	17.904858
37.556375	1585.920906	17.909875
37.260827	1593.812828	17.914893
37.582109	1578.827023	17.919911
37.685611	1593.629242	17.924928
37.418450	1588.019220	17.929946
37.499220	1590.210245	17.934963
37.394318	1587.575323	17.939981
37.549994	1584.414576	17.944999
37.279670	1585.351140	17.950016
37.526862	1588.837049	17.955034
37.908963	1595.746682	17.960051
37.373768	1591.112539	17.965069
37.541034	1582.194755	17.970087
37.958666	1590.457164	17.975104
37.734921	1605.992323	17.980122
38.308939	1606.193798	17.985139
38.186107	1609.830747	17.990157
38.270826	1600.934102	17.995175
38.042550	1601.961736	18.000192
38.109006	1590.112608	18.005210
38.295084	1595.279110	18.010227
37.946819	1601.219529	18.015245
38.260980	1591.123478	18.020263
38.249276	1598.648323	18.025280
38.436784	1602.446086	18.030298
38.452331	1601.697518	18.035315
38.363955	1605.604351	18.040333
38.491825	1602.148598	18.045351
38.396976	1594.169881	18.050368
38.017652	1607.293401	18.055386
38.406355	1596.544846	18.060403
38.072290	1599.790786	18.065421
38.345008	1599.214594	18.070439
38.443083	1599.590155	18.075456
38.453055	1596.921250	18.080474
38.375246	1617.994464	18.085491
38.509924	1626.392722	18.090509
38.874917	1627.167000	18.095527
39.074533	1631.283633	18.100544
39.027782	1631.616641	18.105562
39.108558	1622.315912	18.110579
38.839387	1638.248783	18.115597
39.003545	1621.920053	18.120615
39.286630	1620.312220	18.125632
38.972055	1627.202190	18.130650
39.368583	1621.508634	18.135667
39.021550	1618.879155	18.140685
38.966929	1614.068970	18.145703
39.442608	1618.605634	18.150720
38.849635	1615.853495	18.155738
39.435564	1612.209292	18.160755
39.389755	1621.482317	18.165773
39.530499	1619.416164	18.170791
39.674720	1617.823451	18.175808
39.472840	1614.901827	18.180826
39.704900	1621.858758	18.185843
39.742212	1619.874693	18.190861
39.659051	1623.376335	18.195879
39.988659	1613.647005	18.200896
39.603871	1613.510790	18.205914
40.028321	1610.493327	18.210931
39.504911	1621.488748	18.215949
39.518172	1612.719283	18.220967
39.669237	1612.721110	18.225984
39.425729	1618.001274	18.231002
39.652556	1611.035426	18.236019
39.573237	1619.562030	18.241037
39.522319	1615.522492	18.246055
39.599898	1623.985716	18.251072
39.435019	1639.649351	18.256090
39.898545	1643.778585	18.261107
40.044374	1638.793467	18.266125
40.167804	1640.152630	18.271143
40.442043	1638.710828	18.276160
40.457986	1638.161011	18.281178
40.710091	1632.455146	18.286195
40.708767	1634.938119	18.291213
40.605910	1629.201661	18.296231
40.650508	1631.969550	18.301248
40.513413	1611.915114	18.306266
40.586811	1603.745146	18.311283
40.409308	1605.037995	18.316301
40.546558	1603.323210	18.321319
40.460466	1600.098162	18.326336
40.683321	1615.742451	18.331354
40.269879	1625.203126	18.336371
40.804341	1620.272953	18.341389
40.515315	1623.378368	18.346407
40.898541	1614.877562	18.351424
40.834158	1631.556833	18.356442
40.850835	1618.090331	18.361459
40.785504	1619.617363	18.366477
40.870771	1622.334422	18.371495
41.129093	1609.761380	18.376512
41.113387	1619.361703	18.381530
41.269629	1611.520140	18.386547
41.177541	1618.497674	18.391565
40.784614	1616.811624	18.396583
41.044849	1616.014270	18.401600
40.477499	1622.122864	18.406618
40.970370	1615.290914	18.411635
41.109038	1636.151141	18.416653
41.119002	1652.633871	18.421671
41.339107	1641.980919	18.426688
41.600864	1640.154961	18.431706
41.396866	1642.670709	18.436723
41.624606	1651.870897	18.441741
41.705105	1645.544227	18.446759
41.920960	1648.985732	18.451776
41.641079	1652.429797	18.456794
41.575784	1641.460324	18.461811
41.605014	1650.605980	18.466829
41.543603	1648.905582	18.471847
41.516896	1647.419517	18.476864
41.546736	1649.738670	18.481882
41.826941	1641.972628	18.486899
41.559803	1658.808337	18.491917
41.547400	1646.176945	18.496935
42.000685	1656.421288	18.501952
41.970148	1671.743810	18.506970
42.423326	1668.434570	18.511987
42.507058	1672.521584	18.517005
42.379374	1657.984851	18.522023
42.107085	1649.923676	18.527040
42.010583	1641.895995	18.532058
42.459832	1653.153606	18.537075
42.536899	1660.479923	18.542093
42.343969	1660.739499	18.547111
42.521424	1645.642800	18.552128
42.339726	1641.485540	18.557146
42.500909	1645.140822	18.562163
42.629093	1668.967014	18.567181
42.477013	1659.652064	18.572199
42.851640	1673.435838	18.577216
42.636971	1669.308834	18.582234
42.738630	1673.191697	18.587251
43.051793	1660.792211	18.592269
42.728232	1653.372991	18.597287
42.666086	1638.748652	18.602304
42.609913	1653.834850	18.607322
42.419983	1661.033724	18.612339
42.463149	1656.241585	18.617357
42.371838	1674.802141	18.622375
42.842925	1661.107600	18.627392
42.737627	1673.423199	18.632410
42.785696	1677.792105	18.637427
42.985640	1689.871344	18.642445
42.727028	1699.846588	18.647463
43.032512	1700.359069	18.652480
42.578368	1700.979225	18.657498
42.725814	1707.265950	18.662515
43.311021	1706.171471	18.667533
43.312880	1711.327965	18.672551
43.469208	1723.936111	18.677568
43.070870	1726.612399	18.682586
43.395367	1716.822433	18.687603
43.701827	1716.654433	18.692621
43.581214	1724.260365	18.697639
43.588778	1712.958301	18.702656
43.713363	1717.835025	18.707674
43.432274	1712.417028	18.712691
43.448646	1712.970690	18.717709
43.492663	1717.098938	18.722727
43.897509	1727.689935	18.727744
44.054805	1738.671540	18.732762
44.278251	1729.979411	18.737779
44.033587	1719.935260	18.742797
44.029876	1714.391411	18.747815
43.743454	1707.642005	18.752832
44.124596	1726.074389	18.757850
44.416436	1744.710955	18.762867
44.311293	1742.435892	18.767885
44.101300	1749.404662	18.772903
44.487353	1742.214750	18.777920
44.696096	1737.456587	18.782938
44.674417	1739.995704	18.787955
44.668565	1712.333900	18.792973
44.182335	1706.532155	18.797991
44.433533	1710.343415	18.803008
44.382813	1740.932466	18.808026
44.211748	1730.232414	18.813043
44.862282	1729.540506	18.818061
44.526525	1737.404119	18.823079
44.640360	1736.875886	18.828096
44.503400	1741.653404	18.833114
44.603074	1733.392009	18.838131
44.349287	1737.329021	18.843149
44.221780	1743.256560	18.848167
44.682581	1752.333176	18.853184
44.765510	1763.221994	18.858202
44.946808	1767.029882	18.863219
45.288332	1758.242987	18.868237
45.119362	1771.004250	18.873255
45.448758	1761.133523	18.878272
45.171634	1759.115678	18.883290
45.576810	1763.468783	18.888307
45.421662	1759.755526	18.893325
45.376984	1757.741712	18.898343
45.524221	1755.735096	18.903360
45.289614	1762.350857	18.908378
45.008871	1754.650479	18.913395
45.504644	1757.798411	18.918413
45.357357	1754.296060	18.923431
45.372887	1760.114487	18.928448
45.153932	1767.102072	18.933466
45.572206	1784.309859	18.938483
45.670323	1779.684570	18.943501
45.503596	1791.280503	18.948519
46.024150	1786.870304	18.953536
46.020886	1784.636241	18.958554
45.699633	1777.539811	18.963571
46.162362	1778.756975	18.968589
45.989455	1779.138436	18.973607
46.143620	1774.450717	18.978624
45.925660	1778.654251	18.983642
45.921294	1783.353921	18.988659
46.095688	1780.875870	18.993677
46.098862	1780.212414	18.998695
46.115521	1780.651069	19.003712
46.015737	1785.567329	19.008730
46.341710	1793.645809	19.013747
46.687688	1804.912364	19.018765
46.367327	1803.958775	19.023783
46.797706	1798.365457	19.028800
46.880283	1800.058175	19.033818
47.091618	1776.702479	19.038835
47.024608	1769.125366	19.043853
46.706942	1768.394563	19.048871
47.029666	1763.214364	19.053888
47.107040	1761.146874	19.058906
46.561449	1758.022291	19.063923
47.217408	1763.799240	19.068941
47.019253	1762.237616	19.073959
47.364243	1758.094688	19.078976
46.790174	1764.781227	19.083994
47.107442	1766.271692	19.089011
47.220995	1751.498467	19.094029
46.970753	1759.629824	19.099047
46.872181	1758.879672	19.104064
47.309176	1760.809371	19.109082
47.062570	1767.099559	19.114099
47.322746	1761.939953	19.119117
47.220992	1785.791013	19.124135
47.236603	1787.817658	19.129152
47.300792	1787.383471	19.134170
47.273081	1801.134767	19.139187
47.608504	1786.605089	19.144205
47.448140	1791.429412	19.149223
47.518766	1793.045761	19.154240
47.727732	1787.477692	19.159258
47.477034	1792.149649	19.164275
47.901742	1787.655713	19.169293
47.662565	1790.982831	19.174311
47.716212	1800.140675	19.179328
47.853396	1808.264598	19.184346
48.149849	1824.867397	19.189363
48.316973	1819.689322	19.194381
48.216713	1820.857586	19.199399
48.402557	1818.900082	19.204416
48.209728	1813.413890	19.209434
47.969280	1810.052151	19.214451
48.093056	1811.374264	19.219469
48.297070	1813.787044	19.224487
48.207794	1811.393594	19.229504
48.298284	1818.644927	19.234522
48.480621	1815.619878	19.239539
48.498845	1803.161242	19.244557
48.352673	1809.927736	19.249575
48.144453	1814.841488	19.254592
48.505750	1811.836413	19.259610
48.419639	1816.609866	19.264627
48.318785	1819.476677	19.269645
48.626570	1840.763514	19.274663
49.091434	1841.787807	19.279680
48.995357	1841.723864	19.284698
48.807719	1840.174663	19.289715
48.998035	1833.036806	19.294733
49.002718	1831.045518	19.299751
49.111500	1843.919119	19.304768
49.057591	1838.185109	19.309786
49.026927	1844.288387	19.314803
49.308063	1827.793218	19.319821
49.311934	1844.099204	19.324839
49.515150	1836.878106	19.329856
49.270099	1829.161545	19.334874
49.307062	1835.844575	19.339891
49.335015	1830.817102	19.344909
49.405474	1825.669993	19.349927
49.456096	1838.933147	19.354944
49.781950	1828.380670	19.359962
49.431242	1840.537822	19.364979
49.558126	1832.207694	19.369997
49.433720	1837.898138	19.375015
49.686083	1852.078701	19.380032
49.915770	1853.401391	19.385050
49.675505	1855.660968	19.390067
50.140799	1854.922562	19.395085
50.208923	1852.994390	19.400103
49.981507	1859.234191	19.405120
50.313213	1858.000574	19.410138
50.102465	1855.733139	19.415155
50.185713	1846.363361	19.420173
50.181326	1851.254790	19.425191
50.233350	1850.909625	19.430208
50.763305	1845.198226	19.435226
50.103916	1852.571382	19.440243
50.448812	1846.506760	19.445261
50.353570	1839.433902	19.450279
50.452052	1846.699673	19.455296
50.680846	1838.212114	19.460314
50.344430	1853.277192	19.465331
50.549296	1840.526592	19.470349
50.558781	1862.204197	19.475367
50.679834	1867.336282	19.480384
51.395272	1866.762759	19.485402
50.848597	1883.444207	19.490419
50.623372	1870.092740	19.495437
50.679986	1879.384000	19.500455
50.495657	1871.702245	19.505472
50.840518	1875.422051	19.510490
50.965173	1883.549663	19.515507
50.989764	1876.917191	19.520525
50.973959	1886.028316	19.525543
51.160708	1899.770567	19.530560
51.480004	1899.158699	19.535578
51.665843	1903.912738	19.540595
51.678133	1903.474937	19.545613
51.835422	1897.412227	19.550631
51.941695	1902.606221	19.555648
52.078086	1884.818397	19.560666
51.731881	1871.483812	19.565683
51.849098	1860.575301	19.570701
52.131380	1858.141973	19.575719
51.726174	1861.144623	19.580736
51.485422	1853.769469	19.585754
51.712595	1868.636120	19.590771
51.786283	1872.316575	19.595789
51.933939	1887.867683	19.600807
52.055953	1892.979145	19.605824
52.312358	1896.415960	19.610842
51.975205	1893.771016	19.615859
52.048382	1885.782436	19.620877
52.496930	1893.039871	19.625895
52.121501	1887.292938	19.630912
52.098752	1880.446251	19.635930
52.200870	1894.168258	19.640947
52.238312	1893.906217	19.645965
52.540714	1883.959172	19.650983
52.053402	1904.966329	19.656000
52.270222	1887.984885	19.661018
52.201853	1902.404040	19.666035
52.273999	1902.996506	19.671053
52.703440	1905.066848	19.676071
52.585268	1916.781216	19.681088
52.636743	1908.337941	19.686106
52.469817	1913.046850	19.691123
52.616989	1917.528157	19.696141
52.930252	1926.538753	19.701159
53.217136	1938.990808	19.706176
53.160081	1933.554140	19.711194
53.031889	1937.799547	19.716211
53.300878	1929.030867	19.721229
53.498306	1934.573565	19.726247
53.520534	1942.208708	19.731264
53.687092	1931.036854	19.736282
53.347811	1927.145380	19.741299
53.616856	1930.736018	19.746317
53.741514	1919.879779	19.751335
53.808254	1926.272085	19.756352
53.830744	1925.374710	19.761370
53.661296	1920.185403	19.766387
53.655562	1926.638923	19.771405
53.945839	1928.527190	19.776423
53.710445	1926.110278	19.781440
53.978040	1922.486433	19.786458
53.897162	1923.794017	19.791475
53.689509	1922.254815	19.796493
53.916189	1912.668329	19.801511
53.898578	1925.632220	19.806528
54.127551	1934.744970	19.811546
53.958551	1945.148454	19.816563
54.022776	1949.926976	19.821581
54.184684	1958.403586	19.826599
54.191115	1958.388023	19.831616
54.305799	1954.669803	19.836634
54.338540	1957.702318	19.841651
54.292214	1957.064767	19.846669
54.464470	1965.177454	19.851687
54.469071	1981.334641	19.856704
54.814183	1987.557646	19.861722
55.160868	1996.344634	19.866739
54.954145	1984.780603	19.871757
54.868254	1982.835789	19.876775
54.860095	1983.551008	19.881792
55.306912	1983.232203	19.886810
55.249528	1975.423074	19.891827
55.085743	1987.493088	19.896845
55.248220	1975.806117	19.901863
55.004173	1982.031004	19.906880
55.419963	1983.738254	19.911898
55.250900	1982.110764	19.916915
55.227676	1979.331932	19.921933
55.423554	1978.453877	19.926951
55.060014	1977.973185	19.931968
55.225605	1981.030558	19.936986
55.245182	1979.921059	19.942003
55.317905	1999.581247	19.947021
55.343011	2007.323429	19.952039
55.385417	2017.406122	19.957056
55.779011	2010.952261	19.962074
55.658635	2018.186634	19.967091
55.639074	2014.802841	19.972109
56.051359	2011.135726	19.977127
55.600195	2009.420689	19.982144
55.910599	2012.563148	19.987162
55.919595	2021.106057	19.992179
56.174191	2035.108461	19.997197
56.661029	2032.062478	20.002215
56.838627	2038.305761	20.007232
56.601758	2018.814579	20.012250
56.581726	2007.370409	20.017267
56.384005	1999.712069	20.022285
56.761994	1996.485292	20.027303
56.280852	2003.181742	20.032320
56.652563	2002.608437	20.037338
56.918241	1997.908092	20.042355
56.376926	2015.694728	20.047373
56.997637	2016.870005	20.052391
57.001449	2032.947454	20.057408
56.814634	2030.616185	20.062426
56.922926	2030.044370	20.067443
56.975660	2034.051570	20.072461
57.185969	2026.145333	20.077479
57.347435	2032.585385	20.082496
57.122244	2033.525131	20.087514
57.339980	2032.391477	20.092531
57.036472	2039.053804	20.097549
57.459029	2026.847338	20.102567
56.939592	2025.201873	20.107584
57.530544	2026.803351	20.112602
57.294541	2019.079290	20.117619
57.288640	2024.189928	20.122637
57.443331	2032.439814	20.127655
57.480890	2046.996685	20.132672
57.633795	2058.431226	20.137690
57.660377	2050.216806	20.142707
57.604446	2061.899716	20.147725
57.947529	2049.192990	20.152743
57.582679	2042.873758	20.157760
57.805115	2039.246340	20.162778
58.376567	2063.380066	20.167795
58.125444	2064.844596	20.172813
57.929100	2060.518777	20.177831
58.077981	2070.713405	20.182848
58.182158	2079.887063	20.187866
58.461760	2077.223430	20.192883
58.342868	2070.562663	20.197901
58.825856	2074.794308	20.202919
58.570686	2078.561944	20.207936
58.755231	2080.822473	20.212954
58.991614	2074.251700	20.217971
58.934997	2075.647408	20.222989
58.771945	2065.544241	20.228007
59.025214	2071.993519	20.233024
59.121301	2066.785785	20.238042
59.074710	2060.486684	20.243059
58.835153	2071.066114	20.248077
59.278688	2060.740458	20.253095
59.169926	2065.848456	20.258112
59.444150	2059.691515	20.263130
58.968891	2056.343798	20.268147
59.090100	2064.918153	20.273165
59.249202	2057.712919	20.278183
59.415602	2057.476374	20.283200
59.265831	2066.014495	20.288218
59.253184	2059.332990	20.293235
59.043018	2078.979096	20.298253
59.755140	2078.856525	20.303271
59.810625	2092.096649	20.308288
59.748575	2088.801375	20.313306
59.586159	2084.593557	20.318323
59.046176	2087.109494	20.323341
59.652279	2079.165253	20.328359
59.636406	2094.599941	20.333376
59.667213	2108.220556	20.338394
60.038883	2112.187564	20.343411
59.837209	2114.020301	20.348429
60.351288	2118.531466	20.353447
59.825149	2111.872758	20.358464
60.397116	2107.956732	20.363482
60.652301	2108.794497	20.368499
60.431629	2108.783467	20.373517
60.542650	2105.835135	20.378535
60.508977	2110.431878	20.383552
60.367756	2128.027978	20.388570
60.888851	2133.715586	20.393587
60.705619	2143.816431	20.398605
60.936278	2137.787150	20.403623
61.042535	2140.940603	20.408640
60.670602	2132.101158	20.413658
61.006533	2132.792873	20.418675
61.171062	2132.522384	20.423693
61.133300	2125.288691	20.428711
61.106189	2128.079173	20.433728
60.857680	2129.086567	20.438746
61.327618	2117.689142	20.443763
61.270396	2118.244768	20.448781
61.389383	2125.400578	20.453799
61.452195	2134.080707	20.458816
61.452430	2145.687448	20.463834
61.709228	2144.402038	20.468851
61.685851	2155.573705	20.473869
61.950887	2149.784011	20.478887
62.239807	2146.890862	20.483904
62.040276	2160.468558	20.488922
62.376497	2141.581171	20.493939
62.164445	2144.139278	20.498957
62.216998	2134.702752	20.503975
62.088791	2131.941276	20.508992
62.079871	2144.817688	20.514010
62.308882	2148.785099	20.519027
62.016957	2143.465991	20.524045
62.120595	2151.706677	20.529063
62.451403	2151.071240	20.534080
62.438213	2145.052411	20.539098
62.697567	2139.577847	20.544115
62.595942	2140.888490	20.549133
62.692855	2152.139059	20.554151
62.801436	2152.889681	20.559168
62.319218	2157.999309	20.564186
62.754764	2143.359803	20.569203
62.629888	2155.012860	20.574221
62.860660	2173.383273	20.579239
62.823292	2171.932388	20.584256
62.446314	2173.284298	20.589274
62.927282	2170.705421	20.594291
63.046649	2176.330819	20.599309
63.036945	2181.619704	20.604327
63.403650	2187.059658	20.609344
63.632718	2194.612643	20.614362
63.657455	2190.312387	20.619379
63.637507	2197.403831	20.624397
63.950175	2202.881873	20.629415
64.185526	2178.582584	20.634432
63.874311	2171.219339	20.639450
64.005600	2166.280163	20.644467
63.914142	2168.456481	20.649485
63.852700	2163.121250	20.654503
64.158211	2156.151974	20.659520
63.830713	2160.378078	20.664538
64.056760	2162.459300	20.669555
64.020151	2166.877800	20.674573
64.272246	2175.276994	20.679591
64.111575	2186.604492	20.684608
63.894282	2189.124890	20.689626
64.423408	2194.783631	20.694643
64.517327	2193.343684	20.699661
64.525906	2192.627345	20.704679
64.570028	2187.830553	20.709696
64.328025	2187.906129	20.714714
64.428497	2182.440140	20.719731
64.688868	2182.767977	20.724749
64.576539	2200.931839	20.729767
65.061481	2194.414744	20.734784
64.722693	2217.977750	20.739802
64.951699	2207.760752	20.744819
65.295621	2214.225788	20.749837
65.082863	2217.050570	20.754855
65.140457	2208.751006	20.759872
64.903351	2214.646870	20.764890
65.135472	2207.207814	20.769907
65.039303	2208.703788	20.774925
65.268561	2228.895063	20.779943
65.541281	2240.984731	20.784960
65.570478	2247.315273	20.789978
66.026236	2238.757236	20.794995
65.984168	2236.770094	20.800013
65.641379	2237.516716	20.805031
66.050289	2236.129731	20.810048
65.967831	2236.471814	20.815066
66.159927	2217.891676	20.820083
66.065722	2226.939996	20.825101
66.058180	2225.124705	20.830119
66.223763	2227.412806	20.835136
65.996760	2238.100117	20.840154
66.256485	2232.231742	20.845171
66.189739	2235.568198	20.850189
65.926389	2243.896867	20.855207
66.467481	2248.186266	20.860224
66.300980	2248.722195	20.865242
66.376457	2246.988827	20.870259
66.537890	2244.876645	20.875277
66.135559	2254.796509	20.880295
66.528793	2264.081475	20.885312
66.141409	2272.412979	20.890330
67.019799	2271.834119	20.895347
66.996678	2277.670164	20.900365
66.870218	2277.519906	20.905383
66.821684	2288.997422	20.910400
67.128306	2302.847352	20.915418
67.475796	2299.765336	20.920435
67.748714	2302.945560	20.925453
67.616969	2300.433076	20.930471
67.768766	2296.170809	20.935488
67.559116	2297.152881	20.940506
67.592894	2300.054183	20.945523
67.821018	2295.007589	20.950541
68.065819	2294.686009	20.955559
67.962009	2293.717790	20.960576
67.889745	2290.419046	20.965594
67.949105	2291.729425	20.970611
68.030596	2289.660002	20.975629
68.007389	2289.087117	20.980647
68.197543	2286.214234	20.985664
68.047973	2291.404657	20.990682
68.113299	2295.003128	20.995699
68.347164	2301.838804	21.000717
68.364693	2315.160997	21.005735
68.512382	2322.549165	21.010752
68.277692	2324.299199	21.015770
68.379685	2322.433868	21.020787
68.867164	2319.108185	21.025805
68.894080	2325.227709	21.030823
68.891464	2320.575630	21.035840
68.845031	2313.235012	21.040858
68.885613	2316.515917	21.045875
69.066289	2315.880530	21.050893
69.005998	2315.977201	21.055911
69.245164	2321.803693	21.060928
69.432504	2319.687605	21.065946
69.064399	2304.860137	21.070963
69.253392	2319.702440	21.075981
69.445100	2342.236017	21.080999
69.744848	2337.792147	21.086016
69.395507	2350.530992	21.091034
69.406204	2341.181591	21.096051
69.740584	2331.965223	21.101069
69.736492	2345.980426	21.106087
69.881641	2333.129858	21.111104
69.881087	2342.742687	21.116122
69.475594	2331.917642	21.121139
70.013938	2348.523473	21.126157
69.948693	2361.071578	21.131175
70.290495	2365.499133	21.136192
70.429803	2362.774033	21.141210
70.296404	2367.390908	21.146227
70.236508	2364.496026	21.151245
70.160141	2364.221718	21.156263
70.319716	2356.792636	21.161280
70.240355	2377.806504	21.166298
70.666508	2391.309933	21.171315
70.840807	2388.214842	21.176333
70.847408	2391.294293	21.181351
71.174973	2393.205973	21.186368
71.024306	2378.836945	21.191386
70.964736	2377.042850	21.196403
71.277957	2382.341722	21.201421
71.064203	2379.324667	21.206439
71.494028	2373.069001	21.211456
71.148611	2379.218700	21.216474
71.325127	2384.890620	21.221491
71.415432	2396.589333	21.226509
71.493907	2409.460941	21.231527
71.750938	2417.577939	21.236544
71.931169	2419.377397	21.241562
71.855532	2413.369986	21.246579
71.863995	2417.137358	21.251597
71.813220	2416.056013	21.256615
71.806606	2413.152299	21.261632
71.794321	2405.921344	21.266650
71.814951	2401.463828	21.271667
72.171567	2403.712449	21.276685
72.034993	2429.090419	21.281703
72.193890	2429.871309	21.286720
72.210722	2439.783304	21.291738
71.978516	2436.804335	21.296755
72.257397	2435.267988	21.301773
72.328130	2445.354143	21.306791
72.621387	2456.975593	21.311808
72.748401	2462.351390	21.316826
72.752101	2465.040369	21.321843
73.058199	2468.373804	21.326861
72.816512	2467.952449	21.331879
73.012747	2460.820019	21.336896
73.196909	2462.409765	21.341914
73.227076	2464.241163	21.346931
73.346199	2453.657138	21.351949
73.398761	2464.153816	21.356967
73.513304	2456.998693	21.361984
73.475938	2446.447671	21.367002
73.562732	2451.982101	21.372019
73.877415	2446.138013	21.377037
73.519364	2452.597723	21.382055
73.814653	2453.485171	21.387072
74.019191	2449.727544	21.392090
73.921678	2450.221739	21.397107
74.284374	2450.442871	21.402125
73.672573	2464.704877	21.407143
73.940278	2470.215264	21.412160
73.735252	2487.152612	21.417178
74.055477	2479.294485	21.422195
73.963008	2477.571184	21.427213
74.332133	2470.764867	21.432231
73.863417	2483.125926	21.437248
74.179722	2499.713170	21.442266
74.598410	2506.993951	21.447283
75.289640	2502.729322	21.452301
74.752560	2504.599923	21.457319
75.397068	2492.794165	21.462336
75.377181	2496.441046	21.467354
75.270906	2503.349668	21.472371
75.793799	2494.257906	21.477389
75.404569	2504.875798	21.482407
75.489462	2490.636964	21.487424
75.862332	2496.190187	21.492442
75.514191	2496.879435	21.497459
75.834232	2492.336487	21.502477
75.690335	2485.413130	21.507495
75.595642	2484.025255	21.512512
76.055496	2488.923485	21.517530
75.474979	2493.427019	21.522547
75.727955	2483.448011	21.527565
75.551433	2498.195880	21.532583
75.527462	2495.586380	21.537600
75.581597	2492.215479	21.542618
75.798888	2502.322682	21.547635
76.068953	2513.195609	21.552653
76.023849	2516.123005	21.557671
76.193434	2518.584120	21.562688
76.127701	2512.404154	21.567706
76.016508	2525.806112	21.572723
76.318591	2529.647343	21.577741
76.513675	2541.177625	21.582759
76.749748	2551.226234	21.587776
76.764894	2541.677933	21.592794
76.712102	2545.086165	21.597811
76.851348	2537.836358	21.602829
76.873379	2555.986260	21.607847
77.129752	2567.186708	21.612864
77.484044	2563.879485	21.617882
77.528545	2566.331002	21.622899
77.588035	2563.143463	21.627917
77.454094	2568.413284	21.632935
77.446997	2565.922246	21.637952
77.891044	2566.540566	21.642970
77.634957	2563.995868	21.647987
77.924786	2558.808257	21.653005
77.833902	2557.072872	21.658023
77.933273	2560.306297	21.663040
77.910433	2554.865715	21.668058
77.917673	2567.347649	21.673075
77.951707	2551.835210	21.678093
77.918325	2553.433819	21.683111
78.223493	2561.380707	21.688128
78.067714	2567.351826	21.693146
78.141867	2580.873939	21.698163
78.228515	2585.037488	21.703181
78.532624	2583.423323	21.708199
78.254207	2588.385950	21.713216
78.700969	2585.053962	21.718234
78.536444	2589.277606	21.723251
79.079615	2595.585001	21.728269
79.041423	2602.715479	21.733287
78.948492	2612.375268	21.738304
79.418043	2602.277643	21.743322
79.031553	2614.155867	21.748339
79.375550	2603.799090	21.753357
79.191731	2601.837340	21.758375
79.106943	2603.306662	21.763392
79.305770	2599.917292	21.768410
79.281788	2608.012805	21.773427
79.441307	2617.754034	21.778445
79.648128	2636.392758	21.783463
79.177865	2628.741041	21.788480
79.901552	2629.890659	21.793498
79.772287	2639.241500	21.798515
80.183852	2629.893665	21.803533
80.066450	2635.787584	21.808551
80.484893	2653.831015	21.813568
80.474317	2653.261537	21.818586
80.657960	2651.341306	21.823603
80.736875	2647.439855	21.828621
80.969441	2647.655765	21.833639
80.500195	2647.072857	21.838656
80.469225	2634.167339	21.843674
80.356452	2644.214711	21.848691
80.772592	2642.935165	21.853709
81.161750	2646.161966	21.858727
80.908054	2646.208767	21.863744
81.268803	2646.212888	21.868762
81.047318	2640.692561	21.873779
81.304312	2654.950264	21.878797
81.561446	2669.475692	21.883815
81.236147	2670.638363	21.888832
81.591441	2683.217102	21.893850
81.611097	2675.610234	21.898867
81.696777	2674.222399	21.903885
81.832233	2672.403064	21.908903
81.778378	2677.099780	21.913920
81.770663	2675.227768	21.918938
81.938618	2677.294662	21.923955
82.199415	2667.286288	21.928973
82.166189	2669.286092	21.933991
82.033720	2678.701664	21.939008
82.707917	2695.344040	21.944026
82.346133	2705.995715	21.949043
82.311488	2697.061118	21.954061
82.050410	2704.940804	21.959079
82.110430	2714.033559	21.964096
82.632797	2700.665473	21.969114
82.481522	2716.876795	21.974131
82.730501	2725.094507	21.979149
83.206155	2738.471138	21.984167
82.722706	2741.688496	21.989184
83.293259	2726.948922	21.994202
83.457345	2732.648620	21.999219
83.148795	2720.872142	22.004237
83.369538	2721.297900	22.009255
83.212390	2724.229320	22.014272
83.469164	2720.798044	22.019290
83.112657	2729.831814	22.024307
83.494468	2747.390439	22.029325
83.858858	2747.629802	22.034343
83.897995	2748.798282	22.039360
83.814561	2747.416000	22.044378
83.702071	2742.672136	22.049395
83.853539	2741.484835	22.054413
84.280622	2750.121530	22.059431
84.200225	2768.866242	22.064448
84.429494	2763.555116	22.069466
84.541273	2776.552626	22.074483
84.680494	2764.883877	22.079501
84.734237	2763.865523	22.084519
84.607923	2772.727729	22.089536
84.818078	2771.488579	22.094554
85.130604	2772.455089	22.099571
85.136325	2766.977418	22.104589
84.946416	2769.286270	22.109607
85.075310	2768.797639	22.114624
85.191438	2771.537351	22.119642
85.213148	2769.116714	22.124659
84.978958	2781.400982	22.129677
85.097176	2781.292494	22.134695
85.393338	2793.651962	22.139712
85.234950	2779.952003	22.144730
85.520882	2796.963524	22.149747
85.226791	2810.819666	22.154765
85.612699	2820.741665	22.159783
85.451056	2828.407688	22.164800
85.780273	2825.625470	22.169818
86.041641	2835.979156	22.174835
86.093892	2837.860883	22.179853
86.205913	2837.729797	22.184871
86.219406	2839.461236	22.189888
86.653413	2847.987381	22.194906
86.386095	2851.909980	22.199923
86.378575	2844.953251	22.204941
86.543019	2852.348740	22.209959
86.752213	2868.204447	22.214976
87.236996	2864.257000	22.219994
87.504708	2867.876036	22.225011
87.456187	2867.678611	22.230029
87.665761	2870.037877	22.235047
87.398306	2865.069615	22.240064
87.655391	2857.826134	22.245082
87.738159	2864.685109	22.250099
87.435565	2862.540613	22.255117
87.765447	2857.001755	22.260135
87.926414	2863.602879	22.265152
87.790270	2860.551224	22.270170
87.741606	2858.178842	22.275187
87.721508	2856.399023	22.280205
88.055680	2862.709636	22.285223
88.150271	2861.069895	22.290240
88.033828	2858.321695	22.295258
88.172628	2865.004843	22.300275
88.284880	2877.291277	22.305293
88.574466	2875.210946	22.310311
88.479754	2881.979226	22.315328
88.577944	2883.021394	22.320346
88.688543	2888.558732	22.325363
88.721085	2890.945739	22.330381
88.910331	2881.346747	22.335399
88.643681	2889.196342	22.340416
88.957114	2902.680691	22.345434
89.117065	2917.526011	22.350451
89.114074	2924.129503	22.355469
89.743858	2911.900244	22.360487
88.936207	2926.853419	22.365504
89.475506	2920.091574	22.370522
89.760362	2908.589171	22.375539
89.642415	2910.671937	22.380557
89.462380	2910.139564	22.385575
89.657540	2928.756946	22.390592
89.917440	2930.494844	22.395610
89.866745	2937.900403	22.400627
89.771456	2941.391749	22.405645
90.161767	2936.202338	22.410663
90.272816	2942.015629	22.415680
90.416059	2931.599742	22.420698
90.370947	2943.468939	22.425715
90.578629	2967.206787	22.430733
90.720562	2963.242850	22.435751
91.235172	2962.943520	22.440768
90.801869	2965.456495	22.445786
90.856721	2965.312431	22.450803
90.913615	2958.087483	22.455821
91.064632	2950.571340	22.460839
91.064914	2962.268847	22.465856
91.195529	2957.903994	22.470874
92.039750	2966.693021	22.475891
91.537074	2971.240497	22.480909
91.540167	2967.350733	22.485927
91.524919	2979.283523	22.490944
91.931055	2975.332535	22.495962
91.911380	2971.635533	22.500979
91.522671	2986.196140	22.505997
91.918627	2970.863931	22.511015
91.201792	2981.748218	22.516032
91.607549	2994.324366	22.521050
91.971306	3002.730327	22.526067
91.931421	3008.434370	22.531085
92.453914	3017.736187	22.536103
92.812507	3029.978804	22.541120
92.787173	3023.050144	22.546138
93.134734	3021.374407	22.551155
93.144194	3026.185952	22.556173
93.467653	3018.588857	22.561191
93.247068	3022.209244	22.566208
93.260719	3022.267689	22.571226
93.288823	3023.880971	22.576243
93.174259	3021.631296	22.581261
93.360655	3026.250538	22.586279
93.442668	3025.004631	22.591296
93.127953	3028.924096	22.596314
93.528200	3043.155680	22.601331
93.481453	3056.542305	22.606349
94.072143	3051.396457	22.611367
93.667971	3055.711486	22.616384
93.742985	3060.283032	22.621402
94.007913	3070.846541	22.626419
94.143005	3081.081521	22.631437
94.250406	3072.482279	22.636455
94.042726	3075.216993	22.641472
93.818535	3082.544645	22.646490
94.425908	3086.745348	22.651507
94.084857	3106.471902	22.656525
94.658467	3108.380735	22.661543
94.727662	3104.856407	22.666560
94.835321	3116.767375	22.671578
95.076322	3124.337345	22.676595
95.192223	3130.623177	22.681613
95.543638	3118.329209	22.686631
95.700139	3127.242436	22.691648
95.624651	3123.225079	22.696666
95.891690	3119.426233	22.701683
96.080550	3132.603423	22.706701
96.102956	3121.310872	22.711719
95.965397	3129.645956	22.716736
95.948653	3127.252498	22.721754
96.313006	3124.078153	22.726771
96.117031	3121.359612	22.731789
96.185174	3122.462288	22.736807
96.206015	3122.634515	22.741824
96.190694	3123.509648	22.746842
96.399799	3113.670589	22.751859
96.192134	3129.141995	22.756877
96.100136	3147.108295	22.761895
96.533937	3150.242765	22.766912
96.403082	3157.834553	22.771930
96.532542	3160.649694	22.776947
96.727461	3189.060543	22.781965
96.796046	3182.951388	22.786983
96.483387	3190.127578	22.792000
97.157687	3207.502060	22.797018
97.327409	3205.320261	22.802035
97.322365	3214.079163	22.807053
97.560766	3211.233168	22.812071
97.663829	3220.856550	22.817088
97.744963	3234.347756	22.822106
98.128264	3238.531266	22.827123
98.129332	3245.688218	22.832141
98.398663	3223.582701	22.837159
98.604300	3230.651044	22.842176
98.699485	3233.066319	22.847194
98.701334	3225.634984	22.852211
98.776981	3229.729654	22.857229
98.642686	3223.385148	22.862247
98.865268	3224.724493	22.867264
98.736339	3227.001265	22.872282
98.971057	3215.856976	22.877299
99.114911	3222.237047	22.882317
98.938324	3218.220262	22.887335
99.521266	3235.532335	22.892352
99.169104	3254.686051	22.897370
99.443616	3240.849436	22.902387
99.641437	3247.157582	22.907405
99.913354	3240.444598	22.912423
100.050549	3249.416609	22.917440
99.811726	3243.798139	22.922458
99.549167	3243.508575	22.927475
99.763029	3250.403500	22.932493
99.711191	3261.928346	22.937511
100.292778	3267.416185	22.942528
100.109236	3278.881739	22.947546
100.398655	3276.607663	22.952563
100.222367	3278.996232	22.957581
100.596504	3293.563507	22.962599
100.740578	3294.505575	22.967616
100.844016	3303.723784	22.972634
101.036340	3299.534072	22.977651
100.917548	3296.025077	22.982669
101.096303	3295.959719	22.987687
101.268908	3290.531800	22.992704
101.369380	3295.310247	22.997722
101.891653	3298.447817	23.002739
101.817266	3290.046684	23.007757
101.464925	3299.411623	23.012775
102.010042	3313.573400	23.017792
101.770032	3318.366492	23.022810
102.050797	3313.412050	23.027827
102.146850	3325.045541	23.032845
102.032814	3322.945752	23.037863
102.303812	3317.950007	23.042880
101.869434	3321.090843	23.047898
102.142865	3314.005095	23.052915
102.250529	3322.246916	23.057933
102.074623	3332.033106	23.062951
102.483248	3338.230787	23.067968
102.574822	3349.151965	23.072986
102.789310	3336.913179	23.078003
102.937075	3349.020463	23.083021
102.949084	3360.820669	23.088039
103.177641	3365.403107	23.093056
102.837659	3371.994467	23.098074
103.073556	3364.179000	23.103091
102.935593	3367.852723	23.108109
102.916982	3395.092865	23.113127
103.512630	3397.163460	23.118144
103.436980	3406.789379	23.123162
103.663183	3417.971418	23.128179
103.932818	3425.895497	23.133197
104.042580	3433.035325	23.138215
104.603894	3426.977972	23.143232
104.219735	3430.131383	23.148250
104.719446	3416.566811	23.153267
104.957545	3416.269160	23.158285
104.630892	3410.478536	23.163303
105.228064	3430.196232	23.168320
105.080196	3438.821803	23.173338
105.319112	3438.562997	23.178355
105.581537	3437.310812	23.183373
105.455050	3426.306504	23.188391
105.613986	3426.758661	23.193408
105.264565	3444.133204	23.198426
105.846516	3439.365497	23.203443
105.923203	3447.315234	23.208461
105.574474	3447.205701	23.213479
106.000380	3443.189900	23.218496
105.939424	3449.700050	23.223514
105.737886	3447.413921	23.228531
105.668168	3441.987878	23.233549
105.836959	3453.994507	23.238567
106.096969	3461.350051	23.243584
106.298195	3462.988658	23.248602
106.204569	3462.670724	23.253619
106.641484	3488.251164	23.258637
106.687796	3493.237089	23.263655
107.212150	3491.173720	23.268672
106.935492	3499.942317	23.273690
107.116234	3484.908266	23.278707
107.340562	3490.161602	23.283725
107.385468	3495.840757	23.288743
107.462546	3483.252516	23.293760
107.406771	3498.983818	23.298778
107.718019	3506.738824	23.303795
107.860948	3513.413691	23.308813
108.131905	3521.261607	23.313831
107.926101	3514.744547	23.318848
108.099016	3518.910207	23.323866
108.128893	3512.257264	23.328883
108.181421	3510.377933	23.333901
107.991180	3526.714275	23.338919
108.463357	3535.736512	23.343936
108.381341	3549.420772	23.348954
108.250216	3544.004074	23.353971
108.540608	3546.181145	23.358989
108.814444	3560.517609	23.364007
108.969220	3562.967956	23.369024
109.164399	3565.636839	23.374042
109.061005	3567.988576	23.379059
109.241316	3568.610842	23.384077
109.152130	3567.946065	23.389095
109.458367	3568.456919	23.394112
109.463516	3588.897327	23.399130
109.503251	3595.391259	23.404147
109.963828	3592.476123	23.409165
110.012511	3596.104426	23.414183
110.150472	3594.991355	23.419200
110.239888	3591.794715	23.424218
110.269661	3591.362635	23.429235
110.465731	3600.342031	23.434253
110.386233	3615.635588	23.439271
110.843378	3619.518751	23.444288
110.721463	3622.803211	23.449306
110.911157	3622.775810	23.454323
111.120001	3610.647208	23.459341
111.011793	3616.460828	23.464359
111.060132	3607.047343	23.469376
111.143259	3635.401521	23.474394
111.037950	3639.856224	23.479411
111.377480	3638.277829	23.484429
111.841864	3644.123049	23.489447
112.067098	3633.969929	23.494464
111.935860	3637.816246	23.499482
111.904026	3638.336221	23.504499
111.976860	3652.925764	23.509517
112.012598	3659.413691	23.514535
112.256780	3670.498828	23.519552
112.276450	3673.406266	23.524570
112.464432	3664.166108	23.529587
112.630313	3679.476195	23.534605
112.915042	3683.383589	23.539623
113.141226	3690.303838	23.544640
113.317096	3696.385062	23.549658
113.383308	3695.158257	23.554675
113.461999	3693.692739	23.559693
113.268395	3700.914419	23.564711
113.413090	3689.762256	23.569728
113.419232	3696.571676	23.574746
113.361998	3692.172753	23.579763
113.748155	3706.444291	23.584781
113.439741	3716.397954	23.589799
113.810336	3718.184554	23.594816
113.766296	3709.272983	23.599834
113.799057	3735.910250	23.604851
114.134149	3734.203036	23.609869
114.392158	3747.003891	23.614887
114.642623	3743.149366	23.619904
114.966153	3742.686756	23.624922
114.755572	3734.139407	23.629939
114.870325	3746.652914	23.634957
114.865753	3752.621891	23.639975
115.178506	3745.191596	23.644992
115.400649	3756.484409	23.650010
115.078977	3763.222133	23.655027
115.372901	3758.470520	23.660045
115.299558	3777.199128	23.665063
115.495166	3787.846659	23.670080
115.563787	3787.757797	23.675098
115.945930	3791.523088	23.680115
116.433667	3792.641784	23.685133
116.344057	3801.869019	23.690151
116.456994	3819.849016	23.695168
116.691631	3815.087515	23.700186
116.798004	3818.598035	23.705203
117.038051	3810.427673	23.710221
116.807037	3813.525876	23.715239
116.821504	3816.658644	23.720256
117.159743	3815.300163	23.725274
116.981315	3811.967878	23.730291
117.495577	3813.753934	23.735309
117.265314	3819.543737	23.740327
117.034360	3813.615839	23.745344
117.336832	3813.630011	23.750362
117.352890	3835.734921	23.755379
117.761699	3835.966166	23.760397
117.684763	3846.096577	23.765415
117.666740	3848.508247	23.770432
117.894566	3840.025280	23.775450
117.772809	3862.371975	23.780467
118.093081	3866.218011	23.785485
118.241661	3870.568923	23.790503
118.434050	3869.501554	23.795520
118.758304	3882.475043	23.800538
118.399259	3897.317843	23.805555
119.135553	3884.729598	23.810573
118.729826	3892.745259	23.815591
118.998459	3896.959749	23.820608
119.136911	3912.667576	23.825626
119.679049	3917.547917	23.830643
119.843311	3919.843971	23.835661
119.744474	3920.547909	23.840679
119.654307	3918.966606	23.845696
119.742501	3914.916826	23.850714
119.999377	3930.403459	23.855731
120.289134	3930.701275	23.860749
120.294550	3942.919610	23.865767
120.682388	3948.924886	23.870784
120.705717	3942.620929	23.875802
120.387450	3945.141783	23.880819
120.712502	3939.039877	23.885837
120.474226	3949.303776	23.890855
120.285574	3972.948119	23.895872
120.735991	3970.947335	23.900890
120.784249	3989.268208	23.905907
121.210767	3994.915862	23.910925
121.271192	3998.950646	23.915943
120.994114	4008.480736	23.920960
121.663269	4021.355497	23.925978
121.822768	4025.603841	23.930995
122.162975	4025.747614	23.936013
122.323260	4026.411805	23.941031
122.336742	4027.846087	23.946048
122.617473	4020.919863	23.951066
122.304062	4025.174053	23.956083
122.655648	4029.781207	23.961101
122.798091	4042.000557	23.966119
122.790062	4040.759241	23.971136
123.113973	4038.467535	23.976154
123.245387	4046.491993	23.981171
123.081012	4043.083304	23.986189
123.466110	4053.887468	23.991207
123.447453	4049.918346	23.996224
123.902397	4056.233864	24.001242
123.823562	4067.002234	24.006259
123.953649	4061.239697	24.011277
124.207101	4073.786416	24.016295
124.180189	4065.887323	24.021312
124.277068	4067.992162	24.026330
124.300692	4066.507770	24.031347
124.207963	4061.622415	24.036365
124.300530	4070.101420	24.041383
124.454393	4083.211967	24.046400
124.881545	4082.646746	24.051418
124.895638	4098.157205	24.056435
125.107044	4090.309995	24.061453
125.348578	4084.531360	24.066471
125.060928	4092.675628	24.071488
125.449944	4085.421948	24.076506
125.110326	4088.683485	24.081523
125.557453	4102.538533	24.086541
125.374105	4113.510883	24.091559
125.149984	4118.276384	24.096576
125.578394	4127.140044	24.101594
126.042388	4146.241224	24.106611
125.843823	4142.446772	24.111629
126.101841	4143.132588	24.116647
126.437682	4156.606831	24.121664
126.619022	4171.976268	24.126682
126.484069	4176.326957	24.131699
126.663350	4176.143775	24.136717
126.912355	4173.251751	24.141735
126.986558	4189.130363	24.146752
127.409461	4188.947796	24.151770
127.203747	4197.418766	24.156787
127.440945	4198.853038	24.161805
127.797363	4197.272582	24.166823
127.511926	4197.427802	24.171840
128.089715	4205.625723	24.176858
128.086517	4222.118859	24.181875
128.076469	4213.085212	24.186893
128.538727	4215.358748	24.191911
128.317971	4220.924646	24.196928
128.321940	4211.876866	24.201946
128.201553	4236.288386	24.206963
128.444648	4251.610662	24.211981
128.575329	4250.698392	24.216999
128.800940	4257.084251	24.222016
129.401454	4271.391301	24.227034
129.177967	4283.966752	24.232051
129.204655	4279.117473	24.237069
129.135994	4273.668916	24.242087
129.466733	4299.670696	24.247104
129.796964	4303.301769	24.252122
129.912507	4307.455088	24.257139
129.897168	4313.937567	24.262157
130.162507	4324.605814	24.267175
130.262766	4333.084475	24.272192
130.706049	4329.645206	24.277210
130.660705	4333.075432	24.282227
130.977121	4331.468510	24.287245
131.156753	4331.080507	24.292263
130.793621	4331.648663	24.297280
131.125751	4343.418659	24.302298
131.205140	4356.548852	24.307315
131.020320	4357.453693	24.312333
131.575393	4363.700781	24.317351
131.698459	4383.268219	24.322368
131.905339	4376.387143	24.327386
131.742710	4389.788972	24.332403
132.078447	4388.117417	24.337421
132.484865	4382.928808	24.342439
132.184686	4385.938950	24.347456
132.335443	4385.255674	24.352474
132.592124	4395.961630	24.357491
132.614734	4409.261928	24.362509
132.877286	4407.401664	24.367527
132.552989	4408.652493	24.372544
133.468690	4415.265955	24.377562
133.103814	4427.245920	24.382579
133.362571	4432.893947	24.387597
133.680865	4426.055832	24.392615
133.569794	4433.155106	24.397632
133.641222	4424.355925	24.402650
133.786505	4426.701663	24.407667
133.802731	4431.959057	24.412685
134.184984	4442.802552	24.417703
134.621345	4459.284589	24.422720
134.533202	4454.145550	24.427738
134.396880	4446.517182	24.432755
134.634942	4453.041244	24.437773
134.696419	4451.818314	24.442791
134.671153	4460.893523	24.447808
134.835742	4471.333625	24.452826
135.307034	4478.620017	24.457843
134.911958	4481.612811	24.462861
135.072277	4489.905203	24.467879
135.281394	4504.377287	24.472896
135.480750	4508.265555	24.477914
135.586816	4517.526178	24.482931
135.680939	4527.007722	24.487949
136.036634	4534.049450	24.492967
136.289789	4545.319191	24.497984
136.543935	4543.597338	24.503002
136.479705	4540.846890	24.508019
136.791264	4552.202260	24.513037
136.792977	4561.574692	24.518055
136.828016	4575.992971	24.523072
136.999406	4570.227348	24.528090
137.156482	4568.914552	24.533107
137.392210	4578.182095	24.538125
137.407115	4576.984192	24.543143
137.528409	4597.327142	24.548160
137.597780	4592.923542	24.553178
138.025243	4603.429679	24.558195
138.108191	4611.811338	24.563213
138.124895	4610.280000	24.568231
138.270375	4619.515256	24.573248
138.325903	4614.220856	24.578266
138.720488	4628.102397	24.583283
138.739686	4641.784632	24.588301
139.191601	4634.717178	24.593319
139.040041	4635.488942	24.598336
139.354233	4642.224144	24.603354
139.442091	4644.283301	24.608371
139.579599	4649.001689	24.613389
139.745765	4654.506040	24.618407
139.975722	4665.821449	24.623424
140.153130	4668.977026	24.628442
140.058980	4672.297272	24.633459
139.821251	4667.805887	24.638477
140.433203	4674.101963	24.643495
140.086231	4683.989769	24.648512
140.556029	4685.742340	24.653530
140.813431	4687.874240	24.658547
140.604340	4695.851449	24.663565
140.687744	4706.097233	24.668583
140.651957	4724.727425	24.673600
141.063209	4724.217585	24.678618
141.215869	4726.088823	24.683635
141.249933	4746.454284	24.688653
142.044458	4744.739811	24.693671
141.845377	4753.030416	24.698688
142.365779	4742.117729	24.703706
142.417362	4737.695770	24.708723
142.403140	4748.548415	24.713741
142.469146	4746.055165	24.718759
142.671832	4764.541177	24.723776
142.723637	4767.602584	24.728794
143.130327	4773.692479	24.733811
142.975476	4769.549622	24.738829
143.253854	4766.717996	24.743847
143.155549	4761.967231	24.748864
143.354429	4765.791062	24.753882
143.511971	4757.077459	24.758899
143.432238	4777.972140	24.763917
143.578212	4785.188103	24.768935
143.389449	4793.483322	24.773952
143.638906	4803.190548	24.778970
143.910228	4820.947792	24.783987
143.845656	4831.320540	24.789005
144.450853	4823.134484	24.794023
144.558419	4845.612753	24.799040
144.356763	4846.466853	24.804058
144.839207	4849.666471	24.809075
144.846082	4856.165972	24.814093
145.434134	4868.376770	24.819111
145.397953	4882.655121	24.824128
145.151733	4886.548736	24.829146
145.981281	4886.861164	24.834163
145.640081	4893.254494	24.839181
145.799238	4904.440035	24.844199
146.059342	4900.734848	24.849216
145.992937	4913.405291	24.854234
146.503961	4921.987953	24.859251
146.309972	4937.397440	24.864269
146.751126	4932.141472	24.869287
147.044597	4942.362869	24.874304
146.944723	4943.017406	24.879322
147.153040	4943.404337	24.884339
147.065658	4966.310414	24.889357
147.263508	4966.914085	24.894375
147.508675	4963.340518	24.899392
147.344932	4968.513690	24.904410
148.040658	4985.659793	24.909427
147.866538	4987.721415	24.914445
148.244151	4987.610137	24.919463
148.389610	4985.239157	24.924480
148.735464	5004.201068	24.929498
148.855108	5010.778834	24.934515
148.881003	5012.081989	24.939533
149.146818	5015.851483	24.944551
149.148626	5010.398091	24.949568
149.120821	5011.346278	24.954586
149.452204	5018.239461	24.959603
149.173634	5033.950511	24.964621
149.790384	5032.229216	24.969639
149.745002	5037.145754	24.974656
149.448584	5038.081709	24.979674
150.194674	5055.704697	24.984691
149.991397	5066.985800	24.989709
150.295806	5063.038542	24.994727
150.466232	5073.278034	24.999744
150.432485	5093.603190	25.004762
150.881395	5095.286023	25.009779
150.598163	5106.248034	25.014797
150.993251	5102.333008	25.019815
150.862773	5122.378874	25.024832
151.092141	5131.897461	25.029850
151.653096	5135.558264	25.034867
151.798062	5150.378649	25.039885
152.343972	5140.448305	25.044903
152.444415	5146.913533	25.049920
152.457556	5142.962498	25.054938
152.690170	5152.353759	25.059955
152.958201	5145.751268	25.064973
152.879346	5149.988188	25.069991
152.737257	5148.839075	25.075008
152.702165	5151.410105	25.080026
153.049770	5156.240352	25.085043
153.061766	5180.040731	25.090061
153.025029	5175.688403	25.095079
153.430278	5179.689240	25.100096
153.392263	5203.129345	25.105114
154.172567	5200.064903	25.110131
153.570247	5208.624916	25.115149
154.141809	5202.611666	25.120167
154.227981	5218.092394	25.125184
154.329563	5236.719350	25.130202
154.344348	5222.456961	25.135219
154.619437	5237.885166	25.140237
154.622608	5253.828593	25.145255
154.853530	5251.583615	25.150272
154.836737	5263.138779	25.155290
155.471008	5271.454715	25.160307
155.429591	5278.022242	25.165325
155.710727	5281.897163	25.170343
155.850718	5285.745836	25.175360
155.801865	5296.077695	25.180378
156.222932	5304.215511	25.185395
156.120391	5311.775294	25.190413
156.613398	5322.485288	25.195431
156.672035	5315.841785	25.200448
156.574911	5340.732380	25.205466
156.734413	5342.474183	25.210483
156.446596	5350.151294	25.215501
156.946071	5360.479836	25.220519
157.117271	5372.910474	25.225536
157.548598	5373.009253	25.230554
157.799445	5385.591321	25.235571
157.695160	5398.187302	25.240589
157.868576	5394.011983	25.245607
158.344014	5390.328526	25.250624
158.070984	5417.096845	25.255642
158.670416	5416.287263	25.260659
158.651686	5412.421772	25.265677
158.997448	5424.692021	25.270695
159.366446	5422.348551	25.275712
159.256399	5435.850462	25.280730
159.687341	5425.847614	25.285747
159.896763	5427.935579	25.290765
159.805689	5425.301258	25.295783
160.308444	5421.417161	25.300800
160.075481	5426.740559	25.305818
160.269652	5421.450501	25.310835
160.313124	5435.710652	25.315853
160.271110	5454.992503	25.320871
160.711434	5444.983364	25.325888
160.684705	5460.898873	25.330906
160.799943	5457.245107	25.335923
160.930872	5476.427468	25.340941
160.915870	5488.621242	25.345959
161.180008	5486.341591	25.350976
161.281661	5507.423010	25.355994
161.469166	5514.627707	25.361011
161.746933	5517.398244	25.366029
161.618616	5529.850240	25.371047
162.050948	5544.565138	25.376064
162.041061	5549.488560	25.381082
162.306908	5571.757361	25.386099
162.726201	5571.114639	25.391117
162.572196	5573.802300	25.396135
163.249467	5580.540017	25.401152
162.856351	5593.071344	25.406170
162.991015	5604.522923	25.411187
163.347297	5596.717928	25.416205
163.428154	5603.178710	25.421223
163.790996	5611.614588	25.426240
163.845022	5635.105466	25.431258
164.234258	5620.950059	25.436275
164.197149	5630.404377	25.441293
164.315778	5646.837879	25.446311
164.655078	5648.485365	25.451328
164.981689	5653.398004	25.456346
164.903204	5649.722709	25.461363
165.120011	5651.006124	25.466381
165.259456	5664.473225	25.471399
165.746216	5676.549418	25.476416
165.490160	5680.935534	25.481434
165.702231	5677.264898	25.486451
166.058179	5690.565435	25.491469
165.645777	5698.629578	25.496487
166.089108	5704.198676	25.501504
166.129890	5709.287821	25.506522
166.343825	5718.117798	25.511539
166.543804	5730.536078	25.516557
166.651327	5742.409683	25.521575
167.015292	5752.506521	25.526592
167.168211	5766.471612	25.531610
167.512685	5769.387097	25.536627
167.689529	5773.762214	25.541645
167.537391	5784.947149	25.546663
167.833475	5793.341407	25.551680
167.736889	5799.689088	25.556698
168.201486	5807.845163	25.561715
168.486956	5819.711419	25.566733
168.441138	5830.707871	25.571751
168.531063	5821.359034	25.576768
168.741896	5854.848248	25.581786
169.073340	5855.962267	25.586803
169.605634	5852.379559	25.591821
169.344366	5857.788911	25.596839
169.756444	5862.039258	25.601856
170.116714	5874.233421	25.606874
170.303461	5875.099669	25.611891
170.663342	5874.794421	25.616909
170.099839	5872.819501	25.621927
170.809164	5881.000470	25.626944
170.764160	5904.490816	25.631962
170.864811	5905.071237	25.636979
171.103563	5901.211043	25.641997
171.070575	5905.697335	25.647015
171.499307	5916.008815	25.652032
171.869845	5918.077261	25.657050
171.398987	5926.573360	25.662067
171.846510	5926.611969	25.667085
171.831637	5945.952147	25.672103
171.926017	5944.542503	25.677120
172.040421	5959.404152	25.682138
172.256702	5972.833592	25.687156
172.959117	5988.465878	25.692173
172.559276	5987.209726	25.697191
172.949095	5996.943286	25.702208
173.090715	6008.401882	25.707226
173.343152	6019.409734	25.712244
173.382143	6008.699540	25.717261
173.313590	6039.135313	25.722279
173.810444	6038.827077	25.727296
173.637178	6051.365686	25.732314
174.048180	6055.507572	25.737332
174.489634	6070.179708	25.742349
174.531578	6077.823053	25.747367
174.710363	6077.670654	25.752384
174.687993	6102.303544	25.757402
174.820976	6098.916062	25.762420
175.019593	6097.610442	25.767437
174.722485	6116.764417	25.772455
175.574396	6129.230242	25.777472
175.398352	6136.399321	25.782490
175.564535	6155.979937	25.787508
176.108888	6157.144582	25.792525
175.946493	6154.965383	25.797543
176.403032	6172.650168	25.802560
176.675503	6187.952929	25.807578
176.822396	6180.573769	25.812596
176.908111	6187.027684	25.817613
177.237342	6206.684550	25.822631
177.013358	6203.635754	25.827648
177.279881	6217.096465	25.832666
177.374611	6238.467492	25.837684
177.720266	6252.237275	25.842701
177.609495	6253.730137	25.847719
178.247832	6261.444964	25.852736
178.293432	6271.212052	25.857754
178.392375	6271.194954	25.862772
178.772377	6281.935340	25.867789
178.630914	6295.608588	25.872807
179.067099	6305.353566	25.877824
179.482959	6313.328941	25.882842
179.321917	6327.452048	25.887860
179.569343	6329.465319	25.892877
179.740024	6336.970906	25.897895
179.990091	6345.999252	25.902912
180.156819	6361.251161	25.907930
180.082499	6364.184109	25.912948
180.409017	6373.752738	25.917965
180.695194	6385.060865	25.922983
180.942391	6391.893765	25.928000
181.072856	6407.655027	25.933018
181.641845	6419.570102	25.938036
181.936408	6409.713665	25.943053
181.781351	6413.649268	25.948071
182.006514	6426.890952	25.953088
182.180731	6434.949714	25.958106
182.512981	6438.234392	25.963124
182.680821	6441.109147	25.968141
182.501497	6444.934566	25.973159
182.920921	6458.538726	25.978176
183.010069	6470.492322	25.983194
182.732697	6464.193032	25.988212
183.501708	6482.437648	25.993229
183.243700	6495.167857	25.998247
183.461838	6488.884192	26.003264
183.743587	6503.876177	26.008282
183.998091	6520.398363	26.013300
184.422120	6532.777819	26.018317
184.383455	6533.249790	26.023335
184.583318	6554.177718	26.028352
184.427978	6550.077004	26.033370
184.599108	6561.379886	26.038388
185.218400	6569.415442	26.043405
185.208418	6583.898931	26.048423
185.448129	6589.473701	26.053440
185.792441	6614.883168	26.058458
185.839788	6615.621307	26.063476
186.141558	6606.989932	26.068493
185.772385	6625.948510	26.073511
186.172766	6632.657698	26.078528
186.530384	6642.697873	26.083546
186.639678	6656.218858	26.088564
187.029286	6659.618537	26.093581
187.108364	6676.935531	26.098599
187.738208	6664.528133	26.103616
187.537501	6672.326935	26.108634
188.067715	6688.746940	26.113652
188.220392	6688.901320	26.118669
188.467650	6692.625458	26.123687
188.671152	6694.160063	26.128704
188.410619	6693.941762	26.133722
188.418690	6703.423897	26.138740
188.792610	6710.642388	26.143757
188.964821	6715.046103	26.148775
188.976326	6717.089817	26.153792
189.418358	6729.191554	26.158810
189.217791	6746.673856	26.163828
189.706892	6744.293773	26.168845
189.546252	6758.752741	26.173863
189.953031	6777.652352	26.178880
190.119312	6771.726095	26.183898
190.099951	6800.579861	26.188916
190.541215	6799.801133	26.193933
190.836085	6816.643038	26.198951
191.075227	6830.754689	26.203968
191.557651	6824.611453	26.208986
191.402382	6847.214061	26.214004
191.388942	6850.014142	26.219021
192.063736	6862.438985	26.224039
191.818945	6861.830544	26.229056
192.302031	6875.759283	26.234074
192.401757	6882.551435	26.239092
192.846397	6881.455501	26.244109
192.724344	6900.666506	26.249127
192.884470	6913.168717	26.254144
193.254402	6908.405951	26.259162
193.421071	6937.976666	26.264180
193.649222	6941.606356	26.269197
193.839972	6947.145249	26.274215
193.934677	6958.672163	26.279232
194.391885	6970.150100	26.284250
194.053729	6977.689819	26.289268
194.508705	6986.485328	26.294285
194.948789	6997.569133	26.299303
195.087068	7005.180436	26.304320
195.537751	6997.652933	26.309338
195.418285	7020.285305	26.314356
195.430034	7016.531739	26.319373
195.968763	7027.114027	26.324391
196.101804	7037.074270	26.329408
196.353086	7047.811283	26.334426
196.545242	7058.248535	26.339444
196.616453	7058.915004	26.344461
196.724896	7063.998110	26.349479
196.922526	7085.779375	26.354496
197.342317	7088.665312	26.359514
197.235492	7084.320124	26.364532
197.308134	7112.514117	26.369549
197.518418	7115.443408	26.374567
197.996272	7124.553429	26.379584
198.271673	7140.580504	26.384602
198.400339	7149.510468	26.389620
198.573119	7149.555188	26.394637
198.731070	7161.371098	26.399655
198.834503	7176.122278	26.404672
199.274859	7182.182336	26.409690
199.158190	7193.707393	26.414708
199.578132	7203.557228	26.419725
199.733230	7206.127037	26.424743
199.508721	7215.482567	26.429760
199.900728	7218.325867	26.434778
200.036682	7230.903222	26.439796
200.539560	7222.864431	26.444813
200.482851	7246.199587	26.449831
200.640344	7255.518682	26.454848
201.072499	7262.038561	26.459866
201.185045	7274.639518	26.464884
201.081199	7287.489771	26.469901
201.546545	7285.710611	26.474919
201.402253	7306.357014	26.479936
202.140765	7308.038628	26.484954
202.123107	7322.019152	26.489972
202.469752	7332.292376	26.494989
202.640612	7350.579521	26.500007
202.565484	7349.932731	26.505024
203.050639	7361.414203	26.510042
202.586695	7372.395085	26.515060
203.002162	7378.500299	26.520077
203.745227	7398.360314	26.525095
203.456453	7411.039632	26.530112
203.723219	7431.543316	26.535130
204.334491	7434.754444	26.540148
204.463268	7455.337716	26.545165
204.638859	7464.385333	26.550183
204.710180	7473.831461	26.555200
205.377882	7483.832653	26.560218
205.494703	7493.952619	26.565236
205.635099	7492.302064	26.570253
205.695593	7496.600035	26.575271
205.944456	7518.050455	26.580288
206.593762	7509.629666	26.585306
206.550435	7515.719514	26.590324
206.571779	7524.891162	26.595341
207.115663	7538.255094	26.600359
207.553623	7543.667412	26.605376
207.567310	7544.003926	26.610394
207.917417	7533.561794	26.615412
207.794706	7559.183211	26.620429
208.189908	7567.912534	26.625447
207.752832	7566.583641	26.630464
208.446629	7570.754734	26.635482
208.534562	7586.328071	26.640500
208.588398	7598.798793	26.645517
208.621994	7601.061884	26.650535
209.052798	7614.450114	26.655552
209.099388	7615.386926	26.660570
209.396765	7640.934991	26.665588
209.336524	7655.089062	26.670605
210.110524	7657.341443	26.675623
210.107421	7679.923979	26.680640
210.445135	7673.737422	26.685658
210.625220	7684.127460	26.690676
210.439558	7702.302311	26.695693
210.988543	7711.628543	26.700711
210.708889	7730.110438	26.705728
211.214120	7729.731477	26.710746
211.300881	7748.840404	26.715764
211.591529	7766.867945	26.720781
212.145787	7763.900327	26.725799
212.111299	7781.344453	26.730816
212.520283	7796.351257	26.735834
212.562373	7802.831958	26.740852
212.481073	7813.604855	26.745869
212.610234	7825.154264	26.750887
213.075646	7847.433401	26.755904
213.413959	7859.668969	26.760922
213.657761	7862.300609	26.765940
213.773534	7884.554970	26.770957
214.190307	7876.750669	26.775975
214.221931	7892.540796	26.780992
214.681109	7892.498722	26.786010
214.999967	7909.147976	26.791028
214.903962	7920.165209	26.796045
215.408084	7921.804563	26.801063
215.428355	7918.233701	26.806080
215.662776	7935.401888	26.811098
215.947818	7945.808593	26.816116
216.038870	7954.587693	26.821133
216.185213	7948.410656	26.826151
216.222561	7968.782865	26.831168
216.418328	7973.306703	26.836186
216.849995	7993.879127	26.841204
216.550263	8007.480791	26.846221
217.282031	8012.935220	26.851239
217.454048	8033.007150	26.856256
217.816988	8038.918872	26.861274
218.030393	8050.731777	26.866292
218.133930	8070.773342	26.871309
218.519268	8069.417750	26.876327
218.148829	8083.165096	26.881344
218.601830	8095.212499	26.886362
218.873205	8100.785713	26.891380
219.035190	8131.429154	26.896397
219.232851	8142.987934	26.901415
219.676278	8149.427544	26.906432
219.485783	8166.446547	26.911450
219.763089	8177.407671	26.916468
219.593142	8199.059892	26.921485
220.575683	8208.598230	26.926503
220.662690	8218.080802	26.931520
221.018894	8242.511753	26.936538
221.138550	8260.649297	26.941556
221.415240	8261.850547	26.946573
221.893825	8270.755511	26.951591
221.937468	8293.567496	26.956608
222.518776	8278.250692	26.961626
222.712250	8304.462965	26.966644
222.673257	8305.258803	26.971661
223.075100	8303.181256	26.976679
222.949712	8324.062165	26.981696
223.159111	8334.608473	26.986714
223.652187	8336.575037	26.991732
223.849516	8355.831024	26.996749
224.361207	8370.155729	27.001767
224.377416	8363.477803	27.006784
224.386329	8382.386899	27.011802
224.692893	8385.755803	27.016820
225.102335	8400.117154	27.021837
224.868256	8414.981285	27.026855
225.188743	8436.537672	27.031872
225.463442	8447.790091	27.036890
225.646013	8450.127897	27.041908
225.395463	8459.926449	27.046925
226.172494	8477.978260	27.051943
226.222393	8487.163065	27.056960
226.557300	8502.683807	27.061978
226.718770	8508.252514	27.066996
226.847315	8528.577253	27.072013
227.246133	8545.789781	27.077031
227.408562	8551.342589	27.082048
227.453499	8576.029607	27.087066
227.803926	8590.396173	27.092084
227.952995	8600.223974	27.097101
228.267117	8608.439500	27.102119
228.448660	8628.947805	27.107136
228.518563	8637.365264	27.112154
228.826406	8642.321335	27.117172
229.163039	8662.102120	27.122189
229.545645	8665.723181	27.127207
229.863194	8689.988699	27.132224
229.965645	8691.089634	27.137242
230.565562	8696.321927	27.142260
230.210894	8703.858884	27.147277
230.680460	8715.449479	27.152295
230.826858	8723.740884	27.157312
230.950438	8739.297627	27.162330
231.480942	8750.381873	27.167348
231.346123	8761.270614	27.172365
231.605374	8774.866257	27.177383
231.768430	8786.821961	27.182400
231.758489	8810.505364	27.187418
232.107248	8814.477891	27.192436
232.353490	8844.432063	27.197453
232.923910	8849.977306	27.202471
233.119216	8876.468295	27.207488
233.165489	8887.476819	27.212506
233.914183	8904.445902	27.217524
233.857315	8920.024028	27.222541
234.263342	8916.438713	27.227559
234.281653	8937.558171	27.232576
234.569164	8942.516914	27.237594
234.922252	8955.908112	27.242612
235.166267	8978.226271	27.247629
235.416934	8978.009959	27.252647
235.358576	8999.677875	27.257664
235.632659	9019.075570	27.262682
235.785927	9022.712622	27.267700
235.958641	9036.330690	27.272717
236.240281	9058.174006	27.277735
236.873834	9075.875268	27.282752
237.029445	9087.141551	27.287770
237.520072	9095.277692	27.292788
237.369815	9110.227061	27.297805
237.779501	9113.886283	27.302823
238.148163	9136.428239	27.307840
238.015508	9142.753282	27.312858
238.305967	9155.231739	27.317876
238.639571	9177.076856	27.322893
239.043787	9188.391075	27.327911
239.387066	9191.107306	27.332928
239.429348	9211.999427	27.337946
239.839770	9226.368452	27.342964
239.837343	9235.953089	27.347981
240.100233	9239.423939	27.352999
240.347593	9257.004993	27.358016
240.250877	9273.870995	27.363034
240.732347	9280.564738	27.368052
241.167865	9301.309949	27.373069
241.238947	9321.684596	27.378087
241.584371	9323.074650	27.383104
241.705916	9340.449739	27.388122
241.963132	9338.789900	27.393140
242.584543	9368.693189	27.398157
242.846768	9372.380821	27.403175
243.065601	9382.087264	27.408192
242.793168	9393.862632	27.413210
243.145506	9398.835208	27.418228
243.415524	9414.670878	27.423245
243.546735	9431.936539	27.428263
244.206247	9444.203660	27.433280
244.122760	9468.170421	27.438298
244.435867	9467.910682	27.443316
244.570479	9488.327806	27.448333
244.723039	9492.890742	27.453351
245.264978	9508.915467	27.458368
245.252598	9525.435321	27.463386
245.953005	9522.543249	27.468404
245.744404	9535.651348	27.473421
246.173292	9550.972419	27.478439
246.454536	9561.625814	27.483456
246.420164	9571.700435	27.488474
247.006188	9594.240141	27.493492
246.949065	9592.313253	27.498509
247.296581	9607.480047	27.503527
247.495620	9613.330469	27.508544
247.344474	9632.488906	27.513562
247.708590	9645.662211	27.518580
247.961355	9665.771666	27.523597
248.322721	9676.406360	27.528615
248.801201	9695.012383	27.533632
248.542182	9716.951612	27.538650
249.137712	9724.780798	27.543668
249.285530	9747.874610	27.548685
249.791368	9759.688426	27.553703
250.414180	9769.788310	27.558720
250.696402	9790.309797	27.563738
250.863292	9803.512729	27.568756
250.964896	9806.874113	27.573773
251.401004	9821.178759	27.578791
251.644896	9825.194898	27.583808
251.742083	9825.668111	27.588826
251.558210	9835.476155	27.593844
251.992340	9848.946073	27.598861
252.367912	9871.448528	27.603879
252.661234	9884.419464	27.608896
252.822515	9902.930128	27.613914
253.047914	9908.938585	27.618932
253.408157	9924.804729	27.623949
252.736130	9952.680307	27.628967
253.482379	9962.627526	27.633984
253.275548	9994.601608	27.639002
253.638974	10015.228112	27.644020
254.518089	10033.089894	27.649037
254.938235	10052.428422	27.654055
255.417147	10066.895584	27.659072
255.493191	10083.436038	27.664090
255.819589	10095.011159	27.669108
256.106557	10108.515897	27.674125
256.471326	10106.675886	27.679143
256.781156	10122.275619	27.684160
256.892248	10144.806483	27.689178
257.286471	10135.393723	27.694196
257.587673	10159.278137	27.699213
257.467529	10168.345517	27.704231
257.688737	10169.212608	27.709248
257.834391	10195.917253	27.714266
258.116598	10200.189492	27.719284
258.505313	10226.278836	27.724301
258.737543	10240.633364	27.729319
259.208556	10251.273924	27.734336
259.020054	10274.312293	27.739354
259.604169	10284.162864	27.744372
259.571870	10296.843752	27.749389
259.850241	10322.425244	27.754407
260.679381	10322.303030	27.759424
260.560648	10358.296971	27.764442
260.458376	10359.926674	27.769460
260.951497	10381.318442	27.774477
261.362689	10396.361205	27.779495
261.448216	10409.877483	27.784512
261.742253	10423.866627	27.789530
262.072974	10440.091908	27.794548
262.404063	10454.642979	27.799565
262.581975	10460.906886	27.804583
262.881877	10477.194031	27.809600
262.869495	10491.799629	27.814618
263.019230	10512.487356	27.819636
263.210063	10530.001164	27.824653
263.372984	10543.966422	27.829671
263.700037	10564.796614	27.834688
264.032849	10585.685757	27.839706
264.358442	10598.828407	27.844724
264.554732	10608.874159	27.849741
265.003625	10636.125740	27.854759
265.027761	10644.914239	27.859776
265.270040	10668.974612	27.864794
265.884029	10683.426274	27.869812
266.520608	10703.105565	27.874829
266.414550	10722.923568	27.879847
266.961034	10737.761473	27.884864
266.779007	10746.024777	27.889882
266.873018	10764.580657	27.894900
267.405995	10777.843543	27.899917
267.637854	10801.885355	27.904935
268.257557	10814.561930	27.909952
268.167847	10831.331493	27.914970
268.573359	10856.923514	27.919988
269.175405	10871.122056	27.925005
269.154191	10886.172250	27.930023
269.603091	10892.827945	27.935040
269.817892	10921.954482	27.940058
269.915955	10929.262318	27.945076
270.287186	10949.461705	27.950093
270.588133	10967.220908	27.955111
270.983394	10975.292648	27.960128
270.865402	10996.258522	27.965146
271.237643	11012.055209	27.970164
271.660481	11027.060393	27.975181
272.058203	11055.205144	27.980199
272.250007	11058.966279	27.985216
272.546950	11085.033600	27.990234
272.865712	11105.196172	27.995252
273.471292	11108.792705	28.000269
273.475854	11124.240670	28.005287
273.912802	11125.383314	28.010304
273.927008	11142.511027	28.015322
273.992548	11158.689535	28.020340
274.588210	11170.451707	28.025357
274.878841	11178.934808	28.030375
274.859543	11210.888130	28.035392
275.481295	11223.057295	28.040410
275.746863	11244.120726	28.045428
276.153561	11256.763577	28.050445
275.945885	11270.811294	28.055463
276.274847	11281.760479	28.060480
276.758052	11301.158617	28.065498
276.792254	11314.345358	28.070516
277.082177	11328.859124	28.075533
277.377007	11339.134841	28.080551
277.528552	11355.983195	28.085568
277.990180	11378.689394	28.090586
278.267121	11408.725199	28.095604
278.643189	11410.602801	28.100621
278.697427	11428.414380	28.105639
278.986228	11447.988270	28.110656
279.326397	11472.634009	28.115674
279.664051	11479.368243	28.120692
280.033384	11498.802801	28.125709
279.856606	11521.614877	28.130727
280.204968	11534.169904	28.135744
280.704488	11555.382533	28.140762
280.765462	11576.087890	28.145780
281.223589	11583.027564	28.150797
281.141480	11614.467338	28.155815
281.663579	11618.725461	28.160832
281.962882	11633.576745	28.165850
281.999002	11666.223022	28.170868
282.702720	11664.140002	28.175885
282.804149	11688.083385	28.180903
283.230684	11691.782177	28.185920
283.588228	11715.993640	28.190938
283.457066	11733.101917	28.195956
284.182080	11749.078879	28.200973
284.266068	11778.843179	28.205991
284.373534	11779.904892	28.211008
284.654386	11807.545553	28.216026
284.887205	11829.053243	28.221044
285.318028	11857.892000	28.226061
285.383793	11880.606126	28.231079
286.032186	11896.238206	28.236096
286.241426	11908.268165	28.241114
286.644602	11930.761048	28.246132
287.021962	11946.683869	28.251149
287.205287	11962.359903	28.256167
287.027460	11980.520941	28.261184
287.719477	11996.517793	28.266202
288.193158	12022.571552	28.271220
288.679803	12029.464151	28.276237
288.987590	12055.922050	28.281255
289.217507	12063.944490	28.286272
289.853066	12079.717547	28.291290
289.836868	12089.720602	28.296308
290.493183	12103.440073	28.301325
290.542502	12123.919561	28.306343
290.780734	12121.904084	28.311360
291.100027	12130.614591	28.316378
291.297331	12141.409658	28.321396
291.320183	12159.978916	28.326413
291.933995	12176.285153	28.331431
291.982733	12192.533660	28.336448
292.469250	12202.990938	28.341466
292.496732	12223.330763	28.346484
292.681012	12228.462839	28.351501
292.920629	12259.497614	28.356519
293.361595	12269.486566	28.361536
293.409882	12292.489392	28.366554
293.733808	12322.463958	28.371572
294.002295	12334.519096	28.376589
294.595339	12358.823335	28.381607
294.745277	12380.369114	28.386624
295.251174	12393.265911	28.391642
295.412578	12418.845656	28.396660
295.402497	12430.444271	28.401677
296.242584	12464.325359	28.406695
296.244596	12482.841703	28.411712
296.347546	12489.478108	28.416730
296.729937	12527.366917	28.421748
297.179164	12529.328673	28.426765
297.383642	12556.582976	28.431783
297.751556	12583.501397	28.436800
298.172269	12591.768299	28.441818
298.215922	12625.149620	28.446836
298.599844	12629.413552	28.451853
299.033602	12654.021958	28.456871
299.118914	12661.666777	28.461888
299.547082	12684.522178	28.466906
299.554313	12708.069770	28.471924
300.002283	12730.797462	28.476941
300.151961	12748.432372	28.481959
300.981922	12759.512379	28.486976
301.192458	12776.639259	28.491994
300.977133	12796.479454	28.497012
301.577198	12806.031089	28.502029
301.507150	12831.805810	28.507047
302.183264	12852.820710	28.512064
302.596506	12858.685711	28.517082
302.595848	12890.831511	28.522100
302.932809	12900.445664	28.527117
303.295833	12914.504342	28.532135
303.502310	12952.002487	28.537152
303.866568	12953.489824	28.542170
304.097252	12983.707977	28.547188
304.535697	13003.473302	28.552205
304.812867	13022.688553	28.557223
305.290331	13042.767382	28.562240
305.283137	13058.777013	28.567258
305.738984	13087.167823	28.572276
305.878457	13107.811707	28.577293
306.460638	13117.328664	28.582311
306.643792	13150.232522	28.587328
307.197706	13157.371351	28.592346
307.262816	13184.128135	28.597364
308.003156	13196.695216	28.602381
308.007883	13216.370267	28.607399
308.442301	13240.815553	28.612416
308.721622	13249.593166	28.617434
309.080380	13274.766511	28.622452
309.353235	13284.875323	28.627469
309.573557	13307.959848	28.632487
309.918101	13333.745534	28.637504
310.250369	13343.783085	28.642522
310.554612	13369.922212	28.647540
310.584984	13389.883206	28.652557
311.416230	13412.357717	28.657575
311.526923	13431.402435	28.662592
312.144567	13440.899531	28.667610
312.168834	13471.709074	28.672628
312.383842	13491.986346	28.677645
312.536050	13503.409143	28.682663
312.693228	13525.834636	28.687680
313.197895	13536.206246	28.692698
313.087843	13570.982898	28.697716
313.888373	13592.566007	28.702733
314.415972	13614.689182	28.707751
314.329118	13650.103591	28.712768
314.984821	13669.053646	28.717786
315.508215	13689.885302	28.722804
316.090155	13699.500355	28.727821
316.216197	13716.222992	28.732839
315.977744	13721.070912	28.737856
317.177330	13733.663260	28.742874
317.425236	13744.846594	28.747892
317.646870	13757.812018	28.752909
318.137320	13771.692745	28.757927
318.210851	13795.445267	28.762944
318.697591	13797.055828	28.767962
318.877208	13815.210172	28.772980
318.795928	13823.004463	28.777997
318.940239	13845.761911	28.783015
319.197847	13868.612535	28.788032
319.736813	13877.054372	28.793050
319.843796	13913.871442	28.798068
320.096369	13936.045305	28.803085
320.534683	13952.399716	28.808103
320.614159	13986.639975	28.813120
320.718833	14002.991348	28.818138
321.264378	14027.195624	28.823156
321.549140	14056.841016	28.828173
322.068031	14072.064802	28.833191
322.064887	14101.590871	28.838208
322.684406	14120.449727	28.843226
322.908878	14139.351929	28.848244
323.406102	14159.290173	28.853261
323.763781	14173.048223	28.858279
323.755903	14203.516158	28.863296
323.872190	14220.489941	28.868314
324.032227	14245.152362	28.873332
324.506804	14267.614594	28.878349
325.004740	14295.907554	28.883367
325.125779	14322.939056	28.888384
325.779915	14350.560071	28.893402
326.003512	14371.754282	28.898420
326.222773	14404.150345	28.903437
327.013875	14423.498102	28.908455
327.010705	14447.951431	28.913472
327.799719	14465.676230	28.918490
327.993479	14495.810302	28.923508
328.146396	14513.052562	28.928525
328.882062	14533.003806	28.933543
328.637913	14566.904823	28.938560
329.345081	14589.133564	28.943578
329.471659	14603.623706	28.948596
329.766092	14629.983971	28.953613
330.326477	14650.765025	28.958631
330.271596	14677.991720	28.963648
331.077704	14700.677065	28.968666
331.453477	14722.198010	28.973684
331.500748	14746.282508	28.978701
332.222938	14763.985594	28.983719
332.518959	14798.812690	28.988736
332.644682	14806.133450	28.993754
333.360585	14811.477809	28.998772
333.280628	14841.066780	29.003789
333.937420	14861.357736	29.008807
333.802228	14888.829761	29.013824
334.259214	14910.186203	29.018842
335.007978	14929.347706	29.023860
334.991471	14950.520937	29.028877
335.456009	14975.778689	29.033895
335.189276	15001.382903	29.038912
335.948641	15019.349631	29.043930
336.256575	15051.956106	29.048948
336.255059	15078.857829	29.053965
337.156991	15096.854633	29.058983
337.505494	15126.319610	29.064000
337.984144	15148.742974	29.069018
338.304336	15161.344871	29.074036
338.432862	15192.228651	29.079053
339.007676	15206.213271	29.084071
339.019622	15234.608781	29.089088
339.193401	15260.525065	29.094106
339.455397	15273.582731	29.099124
339.531495	15305.927037	29.104141
340.469975	15326.419402	29.109159
340.521717	15362.750797	29.114176
340.781400	15378.675963	29.119194
341.016934	15405.144943	29.124212
341.317206	15432.437041	29.129229
341.932696	15459.429553	29.134247
342.261313	15487.722648	29.139264
342.861223	15503.810709	29.144282
343.397651	15536.509571	29.149300
343.640432	15550.565204	29.154317
343.947329	15564.632304	29.159335
344.271109	15587.157557	29.164352
344.459719	15604.513268	29.169370
344.845128	15621.708754	29.174388
345.113617	15641.401373	29.179405
345.517432	15664.108932	29.184423
345.739929	15687.970357	29.189440
345.935597	15709.815578	29.194458
346.398918	15742.399278	29.199476
346.646610	15756.052344	29.204493
346.958407	15774.689784	29.209511
347.193517	15812.840701	29.214528
347.381586	15827.187766	29.219546
347.959276	15859.713364	29.224564
348.073359	15883.730146	29.229581
348.297016	15915.427045	29.234599
348.476264	15951.290987	29.239616
348.978419	15982.574661	29.244634
349.457636	16011.220444	29.249652
349.883976	16042.163707	29.254669
350.811329	16072.095705	29.259687
350.781781	16094.490985	29.264704
350.898754	16125.318528	29.269722
351.609777	16151.921221	29.274740
351.855907	16186.330773	29.279757
352.202440	16192.622574	29.284775
352.784244	16229.169205	29.289792
353.303113	16246.814550	29.294810
353.930690	16278.894522	29.299828
353.777392	16305.333152	29.304845
354.492981	16319.123612	29.309863
354.712130	16350.155337	29.314880
355.118902	16372.734130	29.319898
355.587625	16381.192047	29.324916
355.559604	16413.738601	29.329933
355.970994	16427.565314	29.334951
356.503845	16465.432020	29.339968
356.785944	16487.065355	29.344986
357.260920	16508.748760	29.350004
357.675678	16531.862381	29.355021
358.112167	16559.288273	29.360039
358.219709	16576.288000	29.365056
358.537307	16594.159336	29.370074
358.867476	16619.512783	29.375092
359.200991	16650.346447	29.380109
359.514301	16672.960035	29.385127
359.658427	16705.645756	29.390144
360.183233	16732.068986	29.395162
360.631187	16759.231648	29.400180
361.057236	16781.711656	29.405197
361.731367	16812.500281	29.410215
362.016694	16830.055649	29.415232
362.089467	16856.590149	29.420250
362.518594	16875.691762	29.425268
362.844006	16909.864285	29.430285
363.370284	16924.162631	29.435303
363.799084	16947.280814	29.440320
363.925365	16980.800747	29.445338
364.457395	16995.659371	29.450356
364.580072	17032.565930	29.455373
365.216480	17047.815591	29.460391
365.506183	17072.813877	29.465408
365.722166	17102.912778	29.470426
366.468820	17124.372325	29.475444
366.541834	17146.071077	29.480461
366.927704	17170.319024	29.485479
367.328472	17203.480286	29.490496
367.681746	17225.339256	29.495514
368.144708	17243.220338	29.500532
368.140012	17271.109787	29.505549
368.599430	17288.928451	29.510567
368.874041	17314.588510	29.515584
369.194982	17335.097319	29.520602
369.962708	17359.495149	29.525620
370.073593	17383.268724	29.530637
370.382008	17408.217128	29.535655
370.534084	17437.665144	29.540672
370.917933	17462.114049	29.545690
371.287566	17479.974578	29.550708
371.691288	17520.183895	29.555725
371.998273	17543.628887	29.560743
372.612633	17573.470389	29.565760
372.737991	17604.885704	29.570778
372.999262	17627.433543	29.575796
373.196403	17669.635270	29.580813
373.572774	17696.155543	29.585831
373.967362	17723.522514	29.590848
374.139029	17766.444381	29.595866
374.595872	17800.497672	29.600884
374.868214	17849.270419	29.605901
375.415144	17880.444653	29.610919
375.951520	17908.594001	29.615936
376.349701	17948.267718	29.620954
377.040420	17972.879400	29.625972
377.595457	18013.200437	29.630989
377.930745	18033.575316	29.636007
378.216292	18060.271996	29.641024
378.557694	18089.286268	29.646042
379.353494	18118.364109	29.651060
379.606972	18151.937865	29.656077
379.707694	18178.175056	29.661095
380.193244	18203.440574	29.666112
380.758107	18230.647778	29.671130
381.132916	18262.757665	29.676148
381.488687	18289.670097	29.681165
381.984405	18309.605735	29.686183
382.148667	18331.476950	29.691200
382.537578	18368.118552	29.696218
382.816362	18397.561482	29.701236
382.882908	18427.474692	29.706253
383.534415	18456.718888	29.711271
383.671409	18495.451852	29.716288
383.986781	18532.437042	29.721306
384.737180	18568.169542	29.726324
385.099196	18591.226975	29.731341
385.518666	18615.141987	29.736359
385.943776	18654.330528	29.741376
386.060467	18692.501356	29.746394
386.785809	18714.426823	29.751412
387.072072	18743.259029	29.756429
387.674057	18778.032820	29.761447
388.461147	18803.112187	29.766464
388.435261	18835.138150	29.771482
388.924082	18858.365720	29.776500
389.112576	18887.327863	29.781517
389.349071	18912.132774	29.786535
389.658331	18943.371982	29.791552
389.881143	18978.521092	29.796570
390.719996	19002.231671	29.801588
390.753191	19047.038447	29.806605
390.917956	19070.239542	29.811623
391.845430	19101.143404	29.816640
392.088124	19136.702603	29.821658
393.124211	19155.701655	29.826676
393.088054	19192.899408	29.831693
393.487071	19218.425147	29.836711
393.865837	19240.110704	29.841728
394.055904	19269.416931	29.846746
394.685318	19293.520460	29.851764
395.205633	19320.847174	29.856781
395.215668	19343.524047	29.861799
395.892872	19365.557661	29.866816
395.700625	19394.531670	29.871834
396.338613	19424.197584	29.876852
396.515106	19460.648139	29.881869
396.795988	19480.716904	29.886887
397.535954	19520.039821	29.891904
397.781644	19555.708196	29.896922
398.476258	19581.910783	29.901940
398.668930	19602.803069	29.906957
399.130065	19649.003676	29.911975
400.050492	19668.916371	29.916992
400.089044	19692.184937	29.922010
400.556861	19716.598028	29.927028
400.650273	19750.258241	29.932045
400.985240	19776.468629	29.937063
401.540689	19809.257898	29.942080
401.775386	19848.805526	29.947098
402.130324	19879.767749	29.952116
402.650119	19908.240111	29.957133
403.022740	19946.461303	29.962151
403.318259	19981.775485	29.967168
403.777163	20028.980224	29.972186
404.362044	20060.830189	29.977204
404.729452	20098.964301	29.982221
405.035377	20127.310040	29.987239
405.537907	20160.055148	29.992256
405.680331	20204.342418	29.997274
406.267150	20235.504989	30.002292
406.883422	20272.559315	30.007309
406.885476	20310.368100	30.012327
407.325841	20346.992904	30.017344
407.918699	20384.680428	30.022362
408.264148	20416.294783	30.027380
408.441451	20462.249770	30.032397
408.635319	20497.335902	30.037415
409.494251	20536.810217	30.042432
409.655267	20582.667322	30.047450
410.565138	20615.628124	30.052468
410.926923	20646.637925	30.057485
411.197016	20677.976714	30.062503
411.953564	20724.249637	30.067520
412.406813	20761.836555	30.072538
412.574814	20783.527456	30.077556
413.211864	20813.276394	30.082573
413.519718	20855.190328	30.087591
414.046862	20873.222350	30.092608
414.432766	20918.216969	30.097626
414.748324	20940.949491	30.102644
415.024196	20970.577163	30.107661
415.422224	21009.195466	30.112679
415.927017	21040.001005	30.117696
416.001898	21079.212178	30.122714
416.689685	21119.875060	30.127732
417.222504	21143.393360	30.132749
417.475817	21190.581772	30.137767
417.812615	21211.195199	30.142784
418.372150	21262.342709	30.147802
418.800912	21292.297251	30.152820
419.585463	21321.773556	30.157837
419.535851	21358.253024	30.162855
420.026207	21392.886732	30.167872
420.653275	21429.013124	30.172890
420.894292	21460.947877	30.177908
421.598065	21486.054517	30.182925
421.792005	21516.579679	30.187943
422.499429	21543.353991	30.192960
422.708857	21580.790723	30.197978
423.259742	21607.021837	30.202996
423.585263	21636.267194	30.208013
423.669102	21664.472524	30.213031
424.206132	21696.672507	30.218048
424.636689	21736.400279	30.223066
424.725282	21759.641340	30.228084
425.029144	21797.247403	30.233101
425.327037	21845.977072	30.238119
425.887830	21882.150091	30.243136
426.243021	21924.482994	30.248154
426.585674	21962.474045	30.253172
427.724675	21999.660101	30.258189
428.010659	22043.900052	30.263207
428.362838	22075.935827	30.268224
428.552319	22107.315836	30.273242
429.118212	22146.490794	30.278260
429.759613	22180.300104	30.283277
430.035245	22227.918179	30.288295
430.365382	22263.620878	30.293312
430.714929	22310.045921	30.298330
431.218788	22342.659441	30.303348
431.512985	22382.297764	30.308365
432.068608	22429.376522	30.313383
432.622156	22474.325459	30.318400
433.120135	22510.740433	30.323418
433.408865	22550.515661	30.328436
433.863492	22583.550923	30.333453
434.031422	22641.997216	30.338471
434.904303	22669.498085	30.343488
435.142433	22707.441874	30.348506
435.376872	22759.772002	30.353524
436.241209	22793.353264	30.358541
436.495368	22837.710929	30.363559
436.962797	22875.666028	30.368576
437.518777	22918.075406	30.373594
437.792283	22961.102466	30.378612
438.610358	23006.439520	30.383629
438.365467	23045.719194	30.388647
439.113121	23084.878852	30.393664
439.517276	23119.904077	30.398682
439.753096	23169.513526	30.403700
440.468854	23225.991505	30.408717
440.541472	23262.738672	30.413735
441.362722	23296.731748	30.418752
441.610164	23345.844638	30.423770
442.106442	23389.677982	30.428788
443.060956	23429.464927	30.433805
443.209590	23469.519370	30.438823
443.354643	23513.080003	30.443840
444.050232	23565.765212	30.448858
444.139505	23603.823939	30.453876
445.047238	23648.955481	30.458893
445.257634	23701.442286	30.463911
445.948632	23736.153227	30.468928
446.215446	23773.993718	30.473946
446.226757	23827.687108	30.478964
446.799651	23862.906708	30.483981
447.218728	23913.249660	30.488999
448.230406	23950.897888	30.494016
448.610778	23993.372120	30.499034
449.183563	24036.606255	30.504052
449.575670	24076.814218	30.509069
449.916648	24124.297465	30.514087
450.357996	24155.139661	30.519104
450.765851	24199.634704	30.524122
451.219281	24236.158513	30.529140
452.159687	24276.777692	30.534157
452.284213	24309.561838	30.539175
452.598613	24342.317778	30.544192
453.176472	24375.966921	30.549210
453.161283	24416.407094	30.554228
453.788970	24449.395255	30.559245
454.292473	24499.451560	30.564263
454.880647	24529.633019	30.569280
455.553648	24580.163003	30.574298
455.678777	24608.837899	30.579316
456.189558	24637.641420	30.584333
456.245070	24684.971603	30.589351
456.641598	24734.658348	30.594368
457.270346	24776.774858	30.599386
457.391440	24828.037185	30.604404
458.029432	24865.266695	30.609421
458.267695	24922.253527	30.614439
459.235059	24963.825572	30.619456
459.918790	25010.759357	30.624474
460.165401	25052.062935	30.629492
460.505783	25096.328603	30.634509
461.076863	25137.894106	30.639527
461.371002	25187.463477	30.644544
462.004963	25226.826651	30.649562
462.197528	25281.743642	30.654580
463.084006	25317.658726	30.659597
463.664290	25366.241314	30.664615
464.445822	25411.340041	30.669632
464.607380	25440.641136	30.674650
465.143562	25494.808018	30.679668
465.810538	25528.466756	30.684685
466.095387	25567.500515	30.689703
466.158449	25617.629812	30.694720
466.820954	25655.831640	30.699738
466.621731	25705.178185	30.704756
467.585024	25736.523541	30.709773
468.299578	25803.976005	30.714791
468.981070	25844.925635	30.719808
469.565677	25875.797686	30.724826
469.795253	25925.666906	30.729844
470.414789	25959.750705	30.734861
471.017339	26004.703968	30.739879
471.249751	26044.842029	30.744896
471.875095	26092.523384	30.749914
471.906020	26135.379327	30.754932
472.707258	26176.909253	30.759949
473.257755	26225.899796	30.764967
473.502382	26265.607358	30.769984
473.987853	26305.499114	30.775002
474.658755	26345.420210	30.780020
475.127769	26386.264342	30.785037
475.487538	26431.271509	30.790055
475.555807	26480.717947	30.795072
476.738442	26515.488798	30.800090
477.254096	26557.801876	30.805108
477.521545	26590.446845	30.810125
478.326361	26640.352265	30.815143
478.491906	26683.786630	30.820160
478.923109	26723.883908	30.825178
479.090364	26767.608408	30.830196
479.645117	26804.426884	30.835213
480.127049	26864.903333	30.840231
480.682980	26906.661723	30.845248
481.238448	26941.925220	30.850266
481.919613	26993.691183	30.855284
482.064719	27026.839856	30.860301
482.317229	27070.137772	30.865319
483.064066	27109.089099	30.870336
483.278979	27147.781540	30.875354
483.806439	27199.907934	30.880372
484.459853	27224.966689	30.885389
484.951243	27275.294887	30.890407
485.032331	27316.202254	30.895424
485.391650	27358.407515	30.900442
485.690177	27423.313708	30.905460
486.208873	27457.063839	30.910477
486.980331	27507.999362	30.915495
487.637022	27554.502902	30.920512
487.997736	27593.964012	30.925530
488.472951	27650.743971	30.930548
488.801810	27694.172766	30.935565
489.466323	27742.908983	30.940583
489.525892	27795.953722	30.945600
490.253155	27846.701966	30.950618
491.332302	27895.133398	30.955636
491.957797	27947.185874	30.960653
492.649890	27992.220965	30.965671
492.747500	28040.730052	30.970688
493.351760	28070.107454	30.975706
493.789603	28122.279837	30.980724
494.143217	28155.566511	30.985741
494.749302	28208.736589	30.990759
495.209605	28261.912026	30.995776
495.647376	28307.643045	31.000794
496.290566	28361.542501	31.005812
496.721942	28400.653036	31.010829
497.459130	28448.410698	31.015847
497.430789	28503.024272	31.020864
498.085424	28543.912172	31.025882
498.354814	28597.344211	31.030900
499.241364	28630.893784	31.035917
499.688276	28691.584287	31.040935
499.937488	28745.203096	31.045952
500.503332	28791.879561	31.050970
501.186325	28841.644265	31.055988
501.246046	28893.187464	31.061005
502.332552	28947.696815	31.066023
502.636446	29001.963569	31.071040
503.268937	29043.966812	31.076058
503.758081	29106.106155	31.081076
504.096899	29146.331572	31.086093
504.600970	29203.932080	31.091111
504.672828	29247.647041	31.096128
505.782993	29298.654796	31.101146
506.386570	29350.894917	31.106164
506.484284	29402.941269	31.111181
507.166910	29446.902701	31.116199
507.406568	29493.423635	31.121216
508.181547	29551.497868	31.126234
508.568403	29612.687365	31.131252
509.309669	29670.824362	31.136269
509.888179	29713.399730	31.141287
510.194270	29770.280822	31.146304
510.954762	29823.133692	31.151322
511.618094	29882.120361	31.156340
511.827037	29917.765882	31.161357
512.566778	29960.002822	31.166375
512.859035	30011.939912	31.171392
513.860767	30065.605453	31.176410
514.242113	30115.650857	31.181428
514.813115	30161.790608	31.186445
515.188174	30202.968434	31.191463
515.551481	30255.396141	31.196480
516.041828	30296.577194	31.201498
516.632442	30348.844518	31.206516
516.794080	30394.267000	31.211533
517.144786	30442.119299	31.216551
517.666941	30489.022062	31.221568
518.840136	30528.648778	31.226586
519.046506	30576.045745	31.231604
519.496365	30612.842294	31.236621
519.954332	30657.673738	31.241639
520.229922	30714.730153	31.246656
521.067306	30757.691162	31.251674
521.357949	30808.580199	31.256692
521.707952	30863.911524	31.261709
522.418982	30911.967355	31.266727
522.648061	30967.836467	31.271744
523.442875	31018.368179	31.276762
523.702490	31076.283469	31.281780
524.429505	31129.089013	31.286797
524.800199	31181.556115	31.291815
525.249413	31248.470897	31.296832
525.877892	31299.248650	31.301850
526.356346	31357.860672	31.306868
526.988592	31408.537148	31.311885
527.655242	31465.480794	31.316903
528.142649	31528.452514	31.321920
528.654022	31577.350952	31.326938
529.143576	31646.832146	31.331956
529.386755	31697.510723	31.336973
530.057356	31752.643479	31.341991
530.269283	31827.800454	31.347008
531.197522	31878.284151	31.352026
531.962678	31945.982308	31.357044
532.266956	31998.481754	31.362061
533.210124	32052.759409	31.367079
533.457593	32116.785804	31.372096
534.090913	32164.280461	31.377114
534.789729	32220.848876	31.382132
534.978025	32289.265416	31.387149
535.690473	32340.224744	31.392167
536.020132	32405.633288	31.397184
536.798929	32462.618382	31.402202
537.496980	32509.166077	31.407220
537.809880	32572.776232	31.412237
538.566910	32616.840548	31.417255
538.819045	32683.250611	31.422272
539.756634	32730.522884	31.427290
540.488223	32794.108728	31.432308
540.745930	32851.282270	31.437325
541.181012	32903.046438	31.442343
541.737773	32963.714536	31.447360
542.058036	33024.661797	31.452378
542.502017	33088.065924	31.457396
543.412099	33134.169947	31.462413
544.412380	33202.809067	31.467431
544.463030	33246.695201	31.472448
545.286044	33300.425389	31.477466
545.616276	33359.879539	31.482484
546.197139	33415.732858	31.487501
546.815625	33471.381319	31.492519
547.476952	33534.119940	31.497536
547.857833	33579.719419	31.502554
548.663546	33639.850030	31.507572
548.778173	33699.441968	31.512589
549.636209	33748.781308	31.517607
549.972138	33805.058211	31.522624
550.634179	33857.456605	31.527642
551.317200	33918.069188	31.532660
551.518483	33976.445379	31.537677
552.412470	34019.335506	31.542695
552.747984	34089.691152	31.547712
553.166502	34138.763473	31.552730
554.065319	34191.309857	31.557748
554.330488	34241.534445	31.562765
554.855780	34279.234980	31.567783
555.448913	34334.789341	31.572800
555.618490	34393.374107	31.577818
556.508487	34444.104947	31.582836
556.627279	34496.756048	31.587853
557.314669	34545.990124	31.592871
557.997178	34609.183452	31.597888
558.515772	34668.891654	31.602906
558.920303	34731.661185	31.607924
559.341299	34790.925185	31.612941
560.279391	34846.098997	31.617959
560.579419	34913.446715	31.622976
561.003335	34980.935138	31.627994
561.732860	35044.920666	31.633012
562.490565	35100.456479	31.638029
562.993021	35155.996827	31.643047
563.177627	35227.827324	31.648064
563.849769	35283.885970	31.653082
564.775239	35356.945151	31.658100
565.175355	35421.469388	31.663117
566.223707	35474.127342	31.668135
566.486027	35536.383537	31.673152
567.327305	35609.498701	31.678170
567.943190	35653.855812	31.683188
568.331418	35721.523342	31.688205
569.155037	35771.965939	31.693223
569.544577	35843.891223	31.698240
570.258455	35900.923265	31.703258
570.446556	35948.110290	31.708276
570.760167	36021.794160	31.713293
571.471794	36078.243257	31.718311
572.188002	36152.880469	31.723328
572.754177	36218.178576	31.728346
573.422813	36273.372945	31.733364
573.848153	36332.997941	31.738381
574.706974	36404.077708	31.743399
575.104042	36460.778885	31.748416
576.038452	36527.434303	31.753434
576.348481	36582.720513	31.758452
576.994542	36652.940102	31.763469
577.736521	36707.931134	31.768487
578.233227	36772.422121	31.773504
578.605506	36845.572546	31.778522
579.599866	36903.839621	31.783540
579.751103	36961.454165	31.788557
580.583486	37019.672662	31.793575
580.709379	37085.283466	31.798592
581.574806	37145.772579	31.803610
582.156109	37213.966092	31.808628
582.642665	37281.534807	31.813645
583.425235	37348.518219	31.818663
584.170596	37416.196116	31.823680
584.479184	37480.572397	31.828698
585.373255	37537.699723	31.833716
585.897478	37596.703335	31.838733
586.380682	37659.766716	31.843751
587.017303	37724.029611	31.848768
587.739740	37786.618267	31.853786
588.764746	37836.307327	31.858804
589.245552	37894.697276	31.863821
589.946239	37946.886525	31.868839
590.329585	37996.912610	31.873856
590.975437	38061.778050	31.878874
591.368817	38115.650512	31.883892
592.047920	38172.070476	31.888909
592.410806	38223.337903	31.893927
593.059273	38278.172399	31.898944
593.541537	38316.769144	31.903962
594.072624	38375.976160	31.908980
594.138222	38438.700986	31.913997
594.955681	38493.082038	31.919015
595.192323	38551.113608	31.924032
595.931305	38621.660017	31.929050
596.406227	38687.398760	31.934068
596.847874	38753.143244	31.939085
597.801387	38826.581087	31.944103
598.179137	38888.798104	31.949120
598.458759	38963.818968	31.954138
599.036593	39020.403512	31.959156
600.042152	39105.270280	31.964173
600.447638	39181.167692	31.969191
601.412922	39254.090771	31.974208
601.904685	39321.066410	31.979226
602.819982	39383.473954	31.984244
602.969988	39459.799903	31.989261
603.769098	39528.767827	31.994279
604.362907	39599.108425	31.999296
605.081308	39660.892893	32.004314
606.005664	39726.728310	32.009332
606.409594	39794.446257	32.014349
606.866800	39871.872146	32.019367
607.460962	39935.455350	32.024384
607.697701	40013.698034	32.029402
608.875668	40079.107625	32.034420
609.247238	40154.572717	32.039437
610.191628	40212.179916	32.044455
610.979644	40276.884466	32.049472
611.483127	40343.596717	32.054490
612.014420	40407.068836	32.059508
612.458622	40487.419552	32.064525
612.954131	40555.977501	32.069543
613.665080	40627.192887	32.074560
614.057701	40704.554037	32.079578
614.865727	40773.544094	32.084596
615.674318	40846.966641	32.089613
616.069946	40915.138362	32.094631
617.113157	40979.298045	32.099648
617.650963	41056.141005	32.104666
618.567964	41124.110429	32.109684
618.832009	41196.064913	32.114701
619.370816	41253.474126	32.119719
620.125567	41327.674642	32.124736
620.730981	41406.780918	32.129754
621.408509	41470.264065	32.134772
622.124457	41543.568954	32.139789
622.713054	41605.428770	32.144807
623.264211	41674.398390	32.149824
623.677849	41753.089570	32.154842
624.202652	41822.297723	32.159860
624.956516	41891.957588	32.164877
625.274654	41970.008810	32.169895
626.092071	42038.626333	32.174912
626.549097	42114.817734	32.179930
627.084840	42189.875633	32.184948
627.913689	42267.758366	32.189965
628.401630	42348.981296	32.194983
629.400333	42420.834765	32.200000
629.651748	42499.950594	32.205018
630.618889	42568.734736	32.210036
631.285777	42651.448002	32.215053
631.712540	42712.207988	32.220071
632.731820	42780.128672	32.225088
632.892372	42867.744642	32.230106
633.653499	42925.182228	32.235124
634.338892	42988.681890	32.240141
634.983872	43056.270846	32.245159
635.597878	43118.286198	32.250176
635.713873	43196.259178	32.255194
636.426065	43258.388201	32.260212
637.392554	43338.787980	32.265229
637.945978	43417.371498	32.270247
638.706168	43474.346798	32.275264
638.792206	43560.734338	32.280282
639.668656	43624.700262	32.285300
639.904609	43690.294243	32.290317
640.673295	43773.791305	32.295335
641.675213	43860.104475	32.300352
642.320948	43931.078084	32.305370
643.068963	44010.853832	32.310388
643.548135	44081.107246	32.315405
644.431623	44161.824253	32.320423
645.419229	44231.757304	32.325440
645.828614	44316.026662	32.330458
646.316451	44381.167751	32.335476
647.134591	44462.626252	32.340493
647.481756	44533.755734	32.345511
648.306801	44607.641916	32.350528
649.189267	44689.308629	32.355546
649.728013	44756.899192	32.360564
650.708674	44838.525047	32.365581
650.976230	44906.533610	32.370599
651.811509	44979.671206	32.375616
651.839980	45061.243997	32.380634
653.005465	45137.422062	32.385652
653.346183	45215.457813	32.390669
653.951528	45302.076885	32.395687
654.621232	45380.358870	32.400704
655.447216	45466.329600	32.405722
656.464244	45545.423178	32.410740
657.052399	45618.559928	32.415757
657.590237	45696.214545	32.420775
658.782197	45769.965638	32.425792
659.203332	45851.701078	32.430810
659.623426	45925.087861	32.435828
660.432902	46001.849349	32.440845
660.924558	46091.696011	32.445863
661.793568	46166.803099	32.450880
661.944151	46241.081990	32.455898
663.061453	46322.492712	32.460916
663.829533	46399.240555	32.465933
664.641047	46482.875165	32.470951
665.451626	46548.718754	32.475968
666.151447	46636.844090	32.480986
666.434155	46703.394494	32.486004
667.174895	46786.208460	32.491021
667.322130	46860.446115	32.496039
668.107169	46930.744790	32.501056
668.942504	47014.826230	32.506074
669.787147	47095.379041	32.511092
670.181890	47173.600234	32.516109
670.816653	47268.585784	32.521127
671.589878	47349.126219	32.526144
672.067011	47422.446188	32.531162
672.724796	47508.182409	32.536180
673.789318	47599.548866	32.541197
674.048535	47681.540024	32.546215
674.805128	47744.873383	32.551232
675.520996	47827.806525	32.556250
676.015011	47914.635943	32.561268
677.229415	47991.903779	32.566285
677.788736	48077.147226	32.571303
678.504586	48138.511636	32.576320
678.547837	48224.131664	32.581338
679.558329	48297.025671	32.586356
680.455354	48361.869559	32.591373
680.932180	48446.427181	32.596391
681.390970	48516.362473	32.601408
682.386818	48598.500983	32.606426
683.034363	48682.526087	32.611444
683.801235	48744.443007	32.616461
683.924865	48831.258897	32.621479
684.759749	48908.789034	32.626496
685.300831	48985.682741	32.631514
686.102208	49062.751616	32.636532
686.675983	49142.479855	32.641549
687.167818	49242.918515	32.646567
687.886693	49323.305699	32.651584
688.854890	49422.103108	32.656602
688.889808	49509.148340	32.661620
690.153549	49603.090739	32.666637
690.348738	49704.316784	32.671655
691.297408	49783.243430	32.676672
692.289589	49881.284364	32.681690
692.961788	49975.421191	32.686708
693.613494	50063.459710	32.691725
694.325456	50154.047031	32.696743
694.832793	50250.575016	32.701760
695.734603	50343.374350	32.706778
696.555641	50425.006311	32.711796
697.457864	50515.753364	32.716813
697.848759	50608.726931	32.721831
698.901383	50686.834642	32.726848
699.444706	50785.873561	32.731866
700.095385	50876.152225	32.736884
701.121156	50963.103252	32.741901
701.655249	51056.920738	32.746919
702.533992	51132.203610	32.751936
703.241633	51225.077194	32.756954
703.805240	51310.703791	32.761972
704.703481	51404.987057	32.766989
705.436791	51498.059853	32.772007
706.037172	51581.470470	32.777024
706.504786	51673.065558	32.782042
707.117247	51760.120114	32.787060
707.911836	51841.080119	32.792077
708.737676	51936.034955	32.797095
709.529135	52027.837157	32.802112
710.407307	52131.919498	32.807130
710.875528	52215.569490	32.812148
711.538526	52301.032374	32.817165
712.004853	52399.409933	32.822183
712.823032	52500.882324	32.827200
713.768670	52587.815960	32.832218
714.298255	52682.128480	32.837236
715.175429	52770.628429	32.842253
716.004773	52865.618794	32.847271
717.171482	52947.235744	32.852288
717.831092	53030.825971	32.857306
718.365222	53124.520716	32.862324
719.199211	53196.805314	32.867341
719.871765	53282.580483	32.872359
720.583326	53366.435219	32.877376
721.200014	53467.674276	32.882394
721.964526	53554.275718	32.887412
723.024999	53631.951670	32.892429
723.328243	53723.457181	32.897447
723.848105	53813.815290	32.902464
724.754389	53895.611948	32.907482
725.212252	53987.017288	32.912500
726.333775	54063.844526	32.917517
726.370174	54146.114671	32.922535
726.884568	54233.082707	32.927552
728.020680	54318.254973	32.932570
728.279282	54409.505683	32.937588
729.268060	54496.409042	32.942605
729.638319	54594.194278	32.947623
730.265802	54699.317370	32.952640
731.009710	54784.531254	32.957658
731.663801	54889.872103	32.962676
732.301846	54986.692482	32.967693
732.916271	55084.066955	32.972711
733.499192	55202.108891	32.977728
734.554291	55305.186744	32.982746
735.130737	55399.731990	32.987764
736.349346	55512.653610	32.992781
736.949064	55610.071010	32.997799
737.726682	55712.817760	33.002816
738.435369	55822.299630	33.007834
739.226119	55917.974549	33.012852
739.914544	56021.167326	33.017869
740.576330	56124.838960	33.022887
741.332039	56233.898270	33.027904
742.136025	56337.414791	33.032922
742.957031	56452.473817	33.037940
744.021671	56554.810932	33.042957
744.357567	56660.991041	33.047975
745.059431	56761.796827	33.052992
746.221942	56871.891852	33.058010
746.585919	56976.862042	33.063028
747.726753	57078.007554	33.068045
748.757389	57185.301446	33.073063
748.985804	57289.992379	33.078080
750.383125	57391.337180	33.083098
750.785464	57492.986106	33.088116
751.791786	57582.844853	33.093133
752.307838	57694.188818	33.098151
752.899716	57797.337222	33.103168
753.570843	57906.008877	33.108186
754.253076	58018.363538	33.113204
755.276179	58116.633126	33.118221
755.717543	58218.127595	33.123239
756.632584	58339.166506	33.128256
757.517707	58450.276658	33.133274
758.277749	58557.869110	33.138292
759.067481	58668.060934	33.143309
759.443151	58783.883203	33.148327
760.267170	58883.788354	33.153344
761.205363	58995.423588	33.158362
761.820726	59116.232342	33.163380
763.028061	59216.600278	33.168397
763.786071	59321.226802	33.173415
764.221244	59434.224283	33.178432
765.218521	59532.795758	33.183450
765.825465	59646.360083	33.188468
766.786034	59756.188297	33.193485
767.497828	59859.093557	33.198503
768.530098	59967.160399	33.203520
769.140541	60073.041308	33.208538
769.700736	60181.042012	33.213556
770.647461	60287.209700	33.218573
771.582221	60385.719817	33.223591
772.615540	60502.011934	33.228608
773.271705	60594.798756	33.233626
774.210300	60704.186988	33.238644
774.825795	60804.211934	33.243661
775.570129	60908.501274	33.248679
776.373283	61001.221390	33.253696
776.879269	61102.637440	33.258714
777.691195	61199.060780	33.263732
778.579779	61295.661510	33.268749
778.979697	61395.655485	33.273767
779.920344	61501.185805	33.278784
780.616510	61588.130325	33.283802
781.272987	61694.517681	33.288820
782.212788	61792.540746	33.293837
782.935817	61896.800726	33.298855
783.383502	62010.000029	33.303872
784.354125	62113.095066	33.308890
784.953202	62221.877574	33.313908
785.573010	62332.420736	33.318925
786.532255	62449.412504	33.323943
787.238817	62558.305430	33.328960
788.170549	62667.168007	33.333978
788.882810	62777.533924	33.338996
790.082623	62886.896923	33.344013
790.821294	62993.953753	33.349031
791.296884	63104.809361	33.354048
792.389825	63209.324537	33.359066
793.283232	63328.873264	33.364084
793.755731	63433.207747	33.369101
794.801311	63552.625139	33.374119
795.379177	63662.044549	33.379136
796.372520	63768.968452	33.384154
796.897307	63892.001205	33.389172
797.792782	64000.124571	33.394189
798.815435	64113.461552	33.399207
799.225067	64237.122249	33.404224
800.414007	64350.104305	33.409242
801.087520	64469.752879	33.414260
802.003267	64586.460503	33.419277
803.100176	64689.566473	33.424295
803.614431	64811.607610	33.429312
804.274894	64919.964281	33.434330
805.129905	65042.993475	33.439348
805.819946	65160.708861	33.444365
806.825091	65266.841986	33.449383
807.512548	65398.100249	33.454400
808.251293	65509.664805	33.459418
808.776656	65634.616935	33.464436
809.852329	65764.846048	33.469453
810.842482	65876.427872	33.474471
811.632855	65997.292320	33.479488
812.713442	66115.138138	33.484506
813.792652	66230.595130	33.489524
814.449819	66347.380649	33.494541
815.237884	66454.143650	33.499559
815.862943	66572.952473	33.504576
816.867200	66693.033220	33.509594
817.745278	66794.523040	33.514612
818.672084	66916.103581	33.519629
819.594030	67024.383630	33.524647
820.067035	67150.200614	33.529664
821.315976	67251.688198	33.534682
822.207747	67369.812526	33.539700
822.884592	67485.848744	33.544717
823.562315	67587.097335	33.549735
824.476674	67709.481130	33.554752
825.474263	67809.141524	33.559770
826.098035	67932.371303	33.564788
827.039143	68039.572237	33.569805
828.040168	68158.732443	33.574823
828.486906	68269.259791	33.579840
829.149975	68370.792747	33.584858
830.127137	68487.986085	33.589876
830.743631	68606.086967	33.594893
831.696152	68718.638460	33.599911
832.388082	68823.425019	33.604928
833.281045	68927.021770	33.609946
834.216936	69040.273225	33.614964
834.753773	69147.186212	33.619981
835.892621	69243.523115	33.624999
836.449016	69368.574390	33.630016
837.469684	69469.446439	33.635034
838.127859	69582.304097	33.640052
838.699305	69692.097378	33.645069
839.583508	69809.503052	33.650087
840.422869	69923.375850	33.655104
841.208628	70037.605891	33.660122
841.802365	70164.053052	33.665140
842.808186	70282.667900	33.670157
843.783424	70411.405655	33.675175
844.554880	70533.310801	33.680192
845.641192	70644.762709	33.685210
846.320134	70766.361990	33.690228
846.995518	70895.841486	33.695245
848.054982	71018.024239	33.700263
848.597664	71149.740409	33.705280
849.748504	71272.624044	33.710298
850.472307	71406.107697	33.715316
851.318368	71523.706105	33.720333
852.429880	71653.794643	33.725351
853.183053	71783.753522	33.730368
853.979805	71910.765459	33.735386
855.170736	72037.567503	33.740404
856.091307	72163.978665	33.745421
856.906326	72282.572840	33.750439
857.468263	72414.742518	33.755456
858.587832	72539.263749	33.760474
859.553837	72658.423127	33.765492
860.287343	72796.915954	33.770509
861.271016	72909.199659	33.775527
862.184564	73034.206803	33.780544
862.736020	73165.535360	33.785562
863.881605	73291.656582	33.790580
864.760145	73418.512030	33.795597
865.858513	73541.973729	33.800615
866.397808	73674.116850	33.805632
867.241457	73790.779303	33.810650
868.244190	73916.092961	33.815668
869.070583	74058.676560	33.820685
870.186004	74170.616103	33.825703
871.104070	74301.764366	33.830720
871.994287	74418.447760	33.835738
872.931324	74554.856310	33.840756
873.430816	74677.772044	33.845773
874.768786	74798.525945	33.850791
875.531755	74921.032641	33.855808
876.311769	75047.135893	33.860826
877.276793	75169.718074	33.865844
878.308762	75290.196402	33.870861
878.998971	75412.110695	33.875879
880.115633	75534.865894	33.880896
881.016442	75662.755238	33.885914
882.259392	75777.116906	33.890932
882.478744	75892.224014	33.895949
883.654406	76015.244092	33.900967
884.495215	76139.243671	33.905984
885.315588	76261.185393	33.911002
886.677008	76368.611043	33.916020
887.212708	76504.800749	33.921037
888.036134	76618.692196	33.926055
888.807297	76740.752218	33.931072
889.395518	76855.575614	33.936090
890.247756	76969.521020	33.941108
891.016704	77104.575248	33.946125
891.777962	77217.695722	33.951143
892.663327	77337.988048	33.956160
893.677760	77456.254564	33.961178
894.562568	77584.543466	33.966196
895.447494	77708.171302	33.971213
896.380959	77822.879328	33.976231
897.103707	77948.774501	33.981248
897.758490	78079.444690	33.986266
898.800014	78200.089033	33.991284
899.594172	78337.018886	33.996301
900.562914	78459.485763	34.001319
901.292228	78596.389969	34.006336
902.180727	78725.247773	34.011354
902.919560	78857.521629	34.016372
903.992552	78999.008168	34.021389
905.177947	79129.501827	34.026407
905.908617	79271.040363	34.031424
906.644387	79400.047478	34.036442
907.998370	79541.155683	34.041460
908.564403	79677.530460	34.046477
909.880269	79807.146140	34.051495
910.753032	79947.096580	34.056512
911.424616	80086.720572	34.061530
912.123631	80227.682012	34.066548
913.171472	80373.141431	34.071565
914.044924	80502.056144	34.076583
915.032503	80642.067799	34.081600
916.210447	80791.759572	34.086618
917.111364	80929.921098	34.091636
917.681010	81078.677851	34.096653
918.902033	81211.961189	34.101671
920.039945	81349.630571	34.106688
920.920847	81500.514873	34.111706
922.169772	81632.372611	34.116724
923.173904	81771.199094	34.121741
924.145585	81905.963832	34.126759
924.708422	82031.724691	34.131776
925.462906	82182.393986	34.136794
926.634826	82313.034695	34.141812
927.310553	82459.644482	34.146829
928.290350	82599.473295	34.151847
929.516727	82745.943233	34.156864
930.286148	82893.824626	34.161882
931.621690	83025.106639	34.166900
932.233845	83159.982480	34.171917
933.039734	83302.349762	34.176935
934.234384	83447.874048	34.181952
935.257725	83581.134249	34.186970
936.055228	83713.217778	34.191988
936.901948	83865.439275	34.197005
937.958063	83996.462996	34.202023
938.789510	84149.789802	34.207040
939.609397	84283.992475	34.212058
940.783464	84428.064750	34.217076
941.733477	84574.503400	34.222093
942.416779	84711.591049	34.227111
943.365976	84857.436850	34.232128
943.935778	84998.904491	34.237146
944.897453	85138.770626	34.242164
946.425670	85302.778037	34.247181
947.075317	85446.544707	34.252199
948.275462	85587.120737	34.257216
948.583203	85738.741259	34.262234
949.908249	85882.000279	34.267252
950.530321	86036.937037	34.272269
951.768564	86177.814041	34.277287
952.770327	86315.320352	34.282304
953.461942	86451.923266	34.287322
954.325797	86590.447452	34.292340
955.485473	86730.676345	34.297357
956.228577	86867.317450	34.302375
957.645536	87010.239103	34.307392
958.190108	87146.313504	34.312410
958.764300	87295.577641	34.317428
959.997607	87430.641211	34.322445
960.890657	87573.190965	34.327463
961.872030	87722.997958	34.332480
962.713693	87875.493151	34.337498
963.917802	88021.240499	34.342516
964.867099	88170.916408	34.347533
965.813310	88328.725587	34.352551
966.677774	88472.772615	34.357568
967.698638	88626.166925	34.362586
968.643941	88774.872730	34.367604
969.446068	88931.507338	34.372621
970.987067	89074.680392	34.377639
971.817994	89233.014572	34.382656
972.569260	89381.477789	34.387674
973.555467	89540.762924	34.392692
974.350896	89695.315211	34.397709
975.384126	89850.025359	34.402727
976.739086	90007.670453	34.407744
977.570897	90170.491406	34.412762
978.566800	90334.868525	34.417780
979.343078	90492.011253	34.422797
980.371386	90652.385358	34.427815
981.144671	90813.998866	34.432832
982.169193	90979.888263	34.437850
983.168787	91148.346169	34.442868
984.281676	91311.596694	34.447885
985.326117	91473.169770	34.452903
986.557057	91641.187789	34.457920
987.477752	91810.036763	34.462938
988.433357	91965.627749	34.467956
989.483495	92129.362517	34.472973
990.074023	92280.863894	34.477991
991.587771	92444.226641	34.483008
992.012315	92616.530465	34.488026
993.694079	92788.785849	34.493044
994.523708	92951.132148	34.498061
995.390259	93112.492344	34.503079
996.646253	93271.795396	34.508096
997.167910	93440.095011	34.513114
998.511303	93605.538153	34.518132
999.521387	93763.568497	34.523149
1000.627549	93931.983711	34.528167
1001.956340	94097.698432	34.533184
1002.653101	94270.184073	34.538202
1004.136600	94429.108871	34.543220
1004.895097	94583.160289	34.548237
1005.724376	94742.283901	34.553255
1007.227889	94904.063250	34.558272
1008.112170	95060.818735	34.563290
1008.921177	95217.150886	34.568308
1009.941758	95377.835794	34.573325
1010.860858	95541.627631	34.578343
1011.883481	95706.220023	34.583360
1012.805989	95862.379212	34.588378
1013.980981	96026.701651	34.593396
1014.697978	96199.184705	34.598413
1015.711856	96361.985069	34.603431
1016.802356	96526.236144	34.608448
1017.928053	96693.571730	34.613466
1018.603133	96847.923181	34.618484
1019.939738	97000.355673	34.623501
1020.686010	97149.550506	34.628519
1021.621823	97306.495174	34.633536
1022.457228	97463.223192	34.638554
1023.221306	97621.483340	34.643572
1024.479576	97782.910420	34.648589
1025.362263	97956.441720	34.653607
1026.372055	98117.120682	34.658624
1027.126787	98289.010428	34.663642
1028.183256	98446.220800	34.668660
1029.292257	98626.790867	34.673677
1030.372017	98793.989737	34.678695
1031.618545	98958.053613	34.683712
1032.343450	99141.159943	34.688730
1033.714933	99311.460515	34.693748
1035.005913	99472.728356	34.698765
1035.363949	99653.024697	34.703783
1036.939844	99823.054307	34.708800
1037.931276	100004.210743	34.713818
1038.832610	100171.600114	34.718836
1040.020780	100343.311779	34.723853
1041.223852	100524.715485	34.728871
1042.589379	100681.616306	34.733888
1043.199979	100866.121486	34.738906
1044.402620	101040.994834	34.743924
1045.612678	101207.295217	34.748941
1046.385010	101387.661882	34.753959
1047.505090	101561.925590	34.758976
1048.540381	101740.934264	34.763994
1049.679574	101913.228028	34.769012
1050.501878	102095.269278	34.774029
1051.621941	102260.780858	34.779047
1052.832831	102437.865773	34.784064
1053.863549	102636.459500	34.789082
1055.151076	102805.309105	34.794100
1056.204978	102980.277143	34.799117
1056.786521	103167.171691	34.804135
1058.123172	103343.323830	34.809152
1059.124531	103517.442996	34.814170
1060.084062	103700.941837	34.819188
1061.179802	103885.040001	34.824205
1062.174112	104079.021878	34.829223
1063.779537	104254.249194	34.834240
1064.485710	104439.910084	34.839258
1065.233331	104628.022396	34.844276
1066.710240	104802.603382	34.849293
1067.951733	104988.964853	34.854311
1069.253548	105169.175124	34.859328
1070.185374	105356.793568	34.864346
1071.422737	105538.942114	34.869364
1072.432405	105713.695032	34.874381
1073.459437	105885.583855	34.879399
1074.875143	106068.669122	34.884416
1075.811260	106254.254065	34.889434
1076.874223	106431.611996	34.894452
1077.703754	106606.476558	34.899469
1079.072041	106791.563153	34.904487
1079.992095	106955.459115	34.909504
1081.216558	107137.937386	34.914522
1082.604202	107312.042991	34.919540
1083.771028	107482.918374	34.924557
1084.614073	107662.892056	34.929575
1085.685848	107822.499720	34.934592
1086.622849	108011.668596	34.939610
1087.810770	108188.916170	34.944628
1088.985474	108356.426521	34.949645
1089.613228	108538.455626	34.954663
1090.846154	108698.839831	34.959680
1091.937157	108885.570028	34.964698
1093.031754	109051.615916	34.969716
1094.254973	109214.069476	34.974733
1095.205609	109378.089119	34.979751
1096.244991	109546.921242	34.984768
1097.214535	109713.777212	34.989786
1098.337391	109892.452741	34.994804
1099.473742	110055.027023	34.999821
1100.200828	110228.221891	35.004839
1101.400466	110401.770423	35.009856
1102.370606	110586.480131	35.014874
1103.364469	110762.547815	35.019892
1104.624408	110937.723899	35.024909
1105.787223	111128.346570	35.029927
1107.002296	111302.417628	35.034944
1107.939288	111483.224460	35.039962
1108.586579	111675.038261	35.044980
1110.402416	111859.249320	35.049997
1111.321372	112048.309809	35.055015
1112.433226	112241.570922	35.060032
1113.539152	112426.485870	35.065050
1114.532242	112617.970325	35.070068
1115.607767	112803.374211	35.075085
1116.433996	112998.676782	35.080103
1117.943391	113196.971623	35.085120
1119.127338	113391.140956	35.090138
1119.940197	113592.201553	35.095156
1121.264802	113775.987101	35.100173
1122.382674	113980.154646	35.105191
1123.201735	114187.502374	35.110208
1124.655672	114377.605093	35.115226
1125.501612	114577.805766	35.120244
1126.986906	114777.674109	35.125261
1127.832353	114985.466780	35.130279
1129.532893	115187.202873	35.135296
1130.649138	115382.854162	35.140314
1131.336783	115576.474465	35.145332
1133.120358	115763.655959	35.150349
1133.974534	115969.680612	35.155367
1135.381271	116160.563317	35.160384
1136.599529	116355.469570	35.165402
1137.425526	116559.019784	35.170420
1138.964407	116747.325171	35.175437
1139.934314	116949.232563	35.180455
1141.319892	117145.041480	35.185472
1142.479061	117334.807264	35.190490
1143.676369	117538.822544	35.195508
1144.750615	117720.470316	35.200525
1145.633603	117916.671676	35.205543
1147.129061	118116.941862	35.210560
1148.385033	118315.314358	35.215578
1149.529465	118509.107030	35.220596
1150.751132	118693.726937	35.225613
1151.723119	118889.071203	35.230631
1153.143603	119083.709067	35.235648
1154.395154	119275.930567	35.240666
1155.388527	119468.778908	35.245684
1156.584200	119658.249767	35.250701
1157.555130	119858.707377	35.255719
1158.807041	120048.272839	35.260736
1159.827836	120233.265169	35.265754
1160.551482	120433.108648	35.270772
1162.175137	120627.190977	35.275789
1163.446356	120827.630905	35.280807
1164.525024	121020.145869	35.285824
1165.901419	121197.292055	35.290842
1166.564599	121406.808424	35.295860
1168.087013	121583.818735	35.300877
1169.210986	121779.131765	35.305895
1170.564999	121955.563853	35.310912
1171.613093	122134.011830	35.315930
1173.113115	122306.480655	35.320948
1174.283724	122475.760686	35.325965
1175.068623	122660.325619	35.330983
1176.165831	122833.953956	35.336000
1177.369476	123024.610990	35.341018
1178.654331	123204.027397	35.346036
1179.842714	123394.790694	35.351053
1180.577757	123576.720807	35.356071
1181.607713	123773.684601	35.361088
1182.976459	123959.846570	35.366106
1183.675618	124158.185602	35.371124
1185.308396	124347.335293	35.376141
1186.625806	124557.361220	35.381159
1187.465454	124752.322384	35.386176
1189.094792	124941.527051	35.391194
1189.861062	125142.396204	35.396212
1190.998460	125344.206579	35.401229
1192.487335	125534.338011	35.406247
1193.656570	125737.818713	35.411264
1194.753227	125941.325441	35.416282
1195.864582	126143.779118	35.421300
1197.007533	126350.018573	35.426317
1198.014893	126569.830923	35.431335
1199.273525	126784.432051	35.436352
1200.580398	126992.220368	35.441370
1201.638636	127206.147771	35.446388
1202.647929	127413.443096	35.451405
1204.169162	127636.169367	35.456423
1205.234938	127848.756412	35.461440
1207.045987	128059.003559	35.466458
1207.953825	128281.759805	35.471476
1209.196866	128496.578167	35.476493
1210.284538	128698.697561	35.481511
1211.606527	128919.235068	35.486528
1213.325975	129137.616953	35.491546
1213.989574	129361.232494	35.496564
1215.259062	129569.715995	35.501581
1216.968073	129786.304152	35.506599
1217.638799	130007.020325	35.511616
1219.011986	130214.831798	35.516634
1220.168305	130440.376349	35.521652
1221.603236	130653.719961	35.526669
1222.928458	130865.739455	35.531687
1224.094177	131094.037849	35.536704
1225.428479	131305.348891	35.541722
1226.572947	131524.425410	35.546740
1227.549924	131731.868607	35.551757
1229.150973	131956.399622	35.556775
1230.086785	132179.888584	35.561792
1231.715587	132390.207339	35.566810
1232.767810	132610.624917	35.571828
1234.335006	132822.908936	35.576845
1235.740160	133038.758061	35.581863
1236.686142	133257.346746	35.586880
1237.761227	133460.132300	35.591898
1238.886413	133684.551159	35.596916
1240.397939	133903.431029	35.601933
1241.289628	134124.151653	35.606951
1242.510423	134342.258481	35.611968
1243.825660	134549.207418	35.616986
1245.449861	134783.275167	35.622004
1246.475347	134996.715160	35.627021
1247.646317	135220.642547	35.632039
1248.921404	135437.315061	35.637056
1250.607176	135646.593135	35.642074
1251.434111	135853.884552	35.647092
1252.764288	136052.016407	35.652109
1253.957856	136251.021478	35.657127
1254.792653	136461.294811	35.662144
1256.213109	136659.237865	35.667162
1257.377472	136870.638411	35.672180
1258.729137	137076.468739	35.677197
1259.831239	137292.763546	35.682215
1260.727791	137500.117087	35.687232
1262.505846	137724.569569	35.692250
1263.246893	137938.481177	35.697268
1264.331811	138165.599655	35.702285
1265.731959	138392.160386	35.707303
1266.822666	138621.867529	35.712320
1268.386949	138846.299407	35.717338
1269.426296	139075.067154	35.722356
1270.534569	139315.807214	35.727373
1271.733677	139539.505213	35.732391
1273.059579	139782.482245	35.737408
1274.698232	140003.980439	35.742426
1275.645800	140246.440024	35.747444
1277.189164	140481.296294	35.752461
1278.670053	140721.033637	35.757479
1280.165961	140962.989190	35.762496
1281.534564	141187.671634	35.767514
1282.493238	141426.954937	35.772532
1283.847805	141655.941364	35.777549
1285.420663	141887.987258	35.782567
1286.555213	142134.588362	35.787584
1287.794595	142359.185607	35.792602
1289.384626	142607.426649	35.797620
1290.729296	142840.936829	35.802637
1291.951178	143070.284153	35.807655
1292.922225	143314.397073	35.812672
1294.162516	143539.749891	35.817690
1295.800922	143791.148874	35.822708
1296.879527	144031.102218	35.827725
1298.326053	144271.731889	35.832743
1299.542785	144517.981000	35.837760
1301.327452	144762.210349	35.842778
1302.320447	144997.479506	35.847796
1303.607669	145237.000669	35.852813
1305.203495	145485.400394	35.857831
1306.412744	145727.283842	35.862848
1307.763620	145955.449004	35.867866
1309.075500	146212.055156	35.872884
1310.366647	146443.429142	35.877901
1312.127236	146675.589402	35.882919
1313.504612	146918.378819	35.887936
1315.103505	147160.042559	35.892954
1316.585423	147385.620529	35.897972
1317.525625	147621.308617	35.902989
1318.888705	147847.936360	35.908007
1320.219581	148091.870001	35.913024
1321.702369	148324.365661	35.918042
1322.801572	148559.171047	35.923060
1323.954811	148792.459725	35.928077
1325.099980	149020.665320	35.933095
1326.470560	149265.297703	35.938112
1327.651550	149503.646811	35.943130
1329.083966	149748.513125	35.948148
1330.597041	149993.976513	35.953165
1331.751328	150230.394116	35.958183
1332.608332	150476.298860	35.963200
1334.321203	150710.940259	35.968218
1335.720126	150958.902109	35.973236
1337.150408	151206.961872	35.978253
1338.653935	151427.385797	35.983271
1339.807411	151660.869842	35.988288
1341.056878	151881.972587	35.993306
1342.465310	152111.485227	35.998324
1343.641871	152332.868997	36.003341
1344.679926	152551.410311	36.008359
1345.853227	152788.373432	36.013376
1347.308093	153022.729241	36.018394
1348.856264	153259.278143	36.023412
1349.956672	153497.158260	36.028429
1351.281126	153729.066429	36.033447
1352.184810	153974.174139	36.038464
1353.641652	154215.399234	36.043482
1354.840472	154467.513980	36.048500
1356.161836	154718.925113	36.053517
1357.629003	154970.656256	36.058535
1359.167576	155230.394168	36.063552
1360.179635	155481.861301	36.068570
1361.482941	155740.246087	36.073588
1362.668091	156001.113036	36.078605
1364.509986	156265.310900	36.083623
1366.167821	156519.011997	36.088640
1367.403305	156779.254140	36.093658
1368.817802	157035.700757	36.098676
1370.145717	157301.702984	36.103693
1371.763822	157560.580334	36.108711
1373.244808	157820.598366	36.113728
1374.472940	158074.101216	36.118746
1376.022544	158342.382509	36.123764
1376.875665	158603.156315	36.128781
1378.747074	158854.020496	36.133799
1380.159324	159124.575099	36.138816
1381.466751	159392.269007	36.143834
1383.112021	159657.257358	36.148852
1384.202678	159918.317441	36.153869
1385.975639	160171.933554	36.158887
1387.110662	160441.032918	36.163904
1388.764019	160694.266020	36.168922
1389.946896	160963.868331	36.173940
1391.592007	161233.383308	36.178957
1393.132162	161484.191335	36.183975
1394.591501	161765.475922	36.188992
1395.944330	162023.283342	36.194010
1397.429881	162271.250473	36.199028
1398.766292	162548.424554	36.204045
1400.519032	162807.731208	36.209063
1401.607227	163063.317645	36.214080
1403.251617	163321.617648	36.219098
1404.777093	163577.160272	36.224116
1406.241449	163842.255679	36.229133
1407.590302	164104.161797	36.234151
1408.632477	164362.123509	36.239168
1410.193509	164627.613780	36.244186
1411.462194	164891.009713	36.249204
1412.693429	165156.836857	36.254221
1414.154881	165421.066931	36.259239
1415.749839	165692.064754	36.264256
1416.914406	165959.151240	36.269274
1418.813168	166218.314648	36.274292
1419.777166	166488.165494	36.279309
1421.657525	166760.226624	36.284327
1423.027426	167011.856255	36.289344
1424.270044	167285.282165	36.294362
1425.656178	167551.161582	36.299380
1427.078463	167823.013057	36.304397
1428.541131	168087.791768	36.309415
1429.725742	168346.907930	36.314432
1431.361257	168623.918810	36.319450
1432.995782	168869.881173	36.324468
1434.195338	169130.902725	36.329485
1435.749491	169370.752181	36.334503
1437.528218	169615.159337	36.339520
1438.807678	169863.761677	36.344538
1440.101930	170100.548995	36.349556
1441.281788	170352.533153	36.354573
1443.051872	170600.220881	36.359591
1444.287138	170846.538998	36.364608
1445.840190	171104.023663	36.369626
1446.963576	171356.454058	36.374644
1448.262926	171625.848529	36.379661
1449.778352	171875.729718	36.384679
1450.956539	172138.231113	36.389696
1452.422367	172414.493291	36.394714
1453.851692	172677.768352	36.399732
1455.113165	172945.920293	36.404749
1456.768066	173220.937658	36.409767
1458.339923	173503.026200	36.414784
1459.422003	173771.453538	36.419802
1461.128660	174039.766476	36.424820
1462.294269	174329.211377	36.429837
1464.203505	174604.918001	36.434855
1465.658119	174893.607837	36.439872
1466.842820	175172.648173	36.444890
1468.561153	175445.243769	36.449908
1470.215490	175740.695250	36.454925
1471.698749	176019.424558	36.459943
1473.063856	176308.340570	36.464960
1474.679207	176580.934083	36.469978
1476.095544	176856.214456	36.474996
1477.598227	177148.831164	36.480013
1478.981581	177430.541979	36.485031
1480.429590	177724.960574	36.490048
1482.059105	178016.749123	36.495066
1483.507809	178302.198024	36.500084
1484.827945	178597.810459	36.505101
1486.695875	178876.517463	36.510119
1488.497154	179163.994385	36.515136
1489.763653	179464.062841	36.520154
1490.942626	179749.513618	36.525172
1492.562514	180033.255837	36.530189
1494.007199	180329.822242	36.535207
1495.961495	180626.509203	36.540224
1497.141267	180923.744673	36.545242
1498.659251	181208.297039	36.550260
1500.195992	181512.978039	36.555277
1501.513290	181804.636465	36.560295
1503.113540	182103.827205	36.565312
1504.312385	182409.051495	36.570330
1506.177296	182704.114833	36.575348
1507.358077	183004.217635	36.580365
1509.004388	183300.450019	36.585383
1510.767116	183601.830809	36.590400
1512.222543	183914.992377	36.595418
1513.653311	184196.693695	36.600436
1514.909086	184510.780175	36.605453
1516.465912	184811.046571	36.610471
1518.204886	185131.454120	36.615488
1519.614124	185441.179425	36.620506
1521.577987	185746.219789	36.625524
1522.688399	186048.115219	36.630541
1524.384856	186350.055065	36.635559
1526.206664	186654.032182	36.640576
1527.684231	186947.430493	36.645594
1529.121096	187238.920285	36.650612
1530.497677	187548.852952	36.655629
1532.106283	187848.809637	36.660647
1533.823713	188137.998123	36.665664
1535.168058	188424.545872	36.670682
1536.827426	188706.282703	36.675700
1538.037976	188990.773514	36.680717
1539.314434	189264.236251	36.685735
1540.727112	189557.176132	36.690752
1541.993187	189843.832609	36.695770
1543.620647	190135.660847	36.700788
1545.276341	190439.570962	36.705805
1546.847148	190731.728833	36.710823
1548.585319	191030.080812	36.715840
1549.514317	191337.403427	36.720858
1551.545752	191634.262741	36.725876
1552.773204	191941.412149	36.730893
1554.296757	192248.742681	36.735911
1555.718977	192554.656968	36.740928
1556.980889	192872.557901	36.745946
1558.755261	193189.779126	36.750964
1560.291892	193516.816459	36.755981
1561.972202	193825.791951	36.760999
1563.732540	194146.498806	36.766016
1564.712043	194474.280611	36.771034
1566.808875	194793.195884	36.776052
1568.289964	195127.639398	36.781069
1569.615523	195439.563191	36.786087
1571.569325	195767.342975	36.791104
1572.942746	196092.021012	36.796122
1574.630931	196415.239440	36.801140
1576.182668	196749.336845	36.806157
1577.600346	197086.276554	36.811175
1579.219959	197417.319127	36.816192
1580.868843	197756.864768	36.821210
1582.581995	198088.910883	36.826228
1584.023777	198433.356713	36.831245
1585.955677	198758.514111	36.836263
1587.716157	199100.765025	36.841280
1589.519880	199435.532423	36.846298
1591.380911	199761.023687	36.851316
1592.950148	200092.925556	36.856333
1594.434010	200426.100053	36.861351
1596.397213	200748.125618	36.866368
1597.663051	201084.335617	36.871386
1599.317229	201406.313659	36.876404
1600.711383	201739.585337	36.881421
1602.694979	202074.221300	36.886439
1604.406171	202396.968863	36.891456
1606.142919	202733.908678	36.896474
1607.663839	203059.141094	36.901492
1609.124072	203389.755776	36.906509
1610.560000	203724.692926	36.911527
1612.692291	204045.562487	36.916544
1614.313100	204388.661665	36.921562
1615.995447	204711.995464	36.926580
1617.577741	205040.832366	36.931597
1619.094892	205363.434395	36.936615
1620.990829	205691.219193	36.941632
1622.631759	206022.069487	36.946650
1624.153088	206353.144107	36.951668
1625.622948	206666.274401	36.956685
1627.395374	206993.234351	36.961703
1629.197904	207325.460175	36.966720
1630.654527	207661.553820	36.971738
1632.505453	207966.207755	36.976756
1634.366820	208303.024472	36.981773
1635.798560	208622.276337	36.986791
1637.334043	208943.163028	36.991808
1638.687093	209269.922136	36.996826
1640.460536	209591.686284	37.001844
1641.717131	209917.562319	37.006861
1643.372369	210229.101176	37.011879
1645.144454	210527.771427	37.016896
1646.430916	210853.569951	37.021914
1648.061619	211159.859250	37.026932
1650.000973	211470.365249	37.031949
1651.294381	211786.794873	37.036967
1652.950645	212101.235559	37.041984
1654.345199	212425.726904	37.047002
1656.136824	212747.487180	37.052020
1657.993467	213074.241064	37.057037
1659.355306	213395.617527	37.062055
1660.923321	213714.980102	37.067072
1662.975320	214061.667381	37.072090
1664.413526	214384.761726	37.077108
1666.247132	214715.436482	37.082125
1667.484431	215043.925151	37.087143
1669.353498	215380.056848	37.092160
1670.778727	215727.844372	37.097178
1672.331675	216075.027919	37.102196
1674.054966	216409.231704	37.107213
1675.663207	216761.183370	37.112231
1677.729538	217106.558749	37.117248
1679.169755	217468.903086	37.122266
1680.859442	217811.549358	37.127284
1682.760361	218161.349610	37.132301
1683.982588	218524.470321	37.137319
1685.639175	218874.618172	37.142336
1687.332200	219250.489887	37.147354
1689.189615	219601.038798	37.152372
1690.719673	219968.609280	37.157389
1692.251225	220345.019565	37.162407
1694.159890	220700.694205	37.167424
1695.734493	221077.150743	37.172442
1697.491901	221440.574077	37.177460
1699.544786	221811.645735	37.182477
1701.159778	222186.296057	37.187495
1702.950047	222566.963706	37.192512
1704.787473	222931.547039	37.197530
1706.318603	223373.650479	37.202548
1708.271546	223744.541767	37.207565
1709.565533	224120.750002	37.212583
1711.997343	224482.090446	37.217600
1713.479563	224861.546486	37.222618
1715.640491	225226.362879	37.227636
1717.357776	225590.517044	37.232653
1718.720531	225969.386648	37.237671
1720.838594	226326.263157	37.242688
1722.556570	226696.414841	37.247706
1724.510753	227067.976390	37.252724
1726.753671	227425.673544	37.257741
1727.961616	227791.594551	37.262759
1729.539306	228147.269913	37.267776
1731.350815	228518.960715	37.272794
1733.024786	228886.636560	37.277812
1735.660483	229243.105249	37.282829
1737.065440	229596.222044	37.287847
1738.766551	229952.008687	37.292864
1740.458275	230313.589157	37.297882
1742.547097	230678.356254	37.302900
1744.368785	231025.946534	37.307917
1745.746676	231389.054752	37.312935
1747.511882	231735.589169	37.317952
1749.733305	232100.998266	37.322970
1751.294151	232455.721832	37.327988
1753.330255	232808.056186	37.333005
1754.989594	233152.452142	37.338023
1756.538551	233514.698826	37.343040
1758.320985	233852.979612	37.348058
1760.204915	234188.551771	37.353076
1761.895105	234509.195110	37.358093
1763.399024	234841.605342	37.363111
1765.418994	235161.230173	37.368128
1767.082938	235492.472148	37.373146
1768.259524	235832.457224	37.378164
1770.283088	236165.114348	37.383181
1772.112610	236505.069044	37.388199
1773.418244	236848.260724	37.393216
1775.435395	237189.049337	37.398234
1776.808910	237533.501138	37.403252
1778.397636	237892.016104	37.408269
1780.207344	238242.518983	37.413287
1782.003073	238600.492991	37.418304
1783.655139	238953.690354	37.423322
1785.435491	239325.918746	37.428340
1787.168520	239677.986256	37.433357
1788.487279	240062.409017	37.438375
1790.017942	240437.068369	37.443392
1792.046314	240821.019599	37.448410
1793.480032	241197.398168	37.453428
1795.783300	241586.893779	37.458445
1797.164892	241977.939385	37.463463
1798.934450	242363.917239	37.468480
1800.932936	242763.549839	37.473498
1802.784305	243164.629898	37.478516
1804.401223	243546.214678	37.483533
1806.213068	243949.563268	37.488551
1808.474518	244346.208080	37.493568
1810.324143	244746.249213	37.498586
1811.861446	245148.298482	37.503604
1813.917624	245538.272469	37.508621
1815.638061	245947.633933	37.513639
1817.684922	246348.660673	37.518656
1819.590636	246756.620787	37.523674
1821.125962	247157.910784	37.528692
1823.001758	247564.225585	37.533709
1825.098364	247972.968447	37.538727
1826.744199	248383.615206	37.543744
1828.688508	248787.506692	37.548762
1830.297119	249192.571744	37.553780
1832.154520	249608.112949	37.558797
1833.924839	250035.811586	37.563815
1836.147824	250441.919414	37.568832
1838.060584	250857.884410	37.573850
1839.155309	251273.095724	37.578868
1841.154894	251683.204285	37.583885
1843.248753	252111.511638	37.588903
1845.091496	252534.602291	37.593920
1847.159319	252958.011678	37.598938
1848.574499	253389.150063	37.603956
1850.926154	253801.284819	37.608973
1852.336808	254225.794143	37.613991
1854.098046	254659.695769	37.619008
1855.920991	255083.121236	37.624026
1857.833869	255513.467096	37.629044
1859.772410	255940.938284	37.634061
1861.920499	256363.624565	37.639079
1863.676753	256792.802686	37.644096
1865.517192	257215.031882	37.649114
1867.365772	257654.280004	37.654132
1869.707600	258072.209545	37.659149
1871.349586	258499.247453	37.664167
1873.211471	258929.018007	37.669184
1875.365845	259353.939015	37.674202
1876.990644	259776.915181	37.679220
1878.469455	260196.282729	37.684237
1880.765896	260620.138576	37.689255
1882.409000	261023.500162	37.694272
1884.425074	261425.555294	37.699290
1886.197598	261834.179173	37.704308
1888.317696	262227.401946	37.709325
1889.807298	262630.483551	37.714343
1891.766203	263045.630241	37.719360
1893.637749	263453.144794	37.724378
1895.275015	263861.790175	37.729396
1896.893507	264270.717874	37.734413
1898.937899	264697.814492	37.739431
1900.904375	265120.071697	37.744448
1902.780561	265548.973747	37.749466
1904.302952	265965.333953	37.754484
1906.891107	266401.992752	37.759501
1908.316952	266827.843589	37.764519
1910.258317	267260.391543	37.769536
1912.178953	267693.247358	37.774554
1913.886990	268129.922910	37.779572
1916.167931	268567.544928	37.784589
1918.091725	269006.749632	37.789607
1919.771687	269445.613062	37.794624
1922.071632	269886.812275	37.799642
1923.553774	270334.547519	37.804660
1925.759523	270777.209136	37.809677
1927.445393	271227.754677	37.814695
1929.366665	271683.036434	37.819712
1931.656637	272135.868781	37.824730
1933.424050	272587.872241	37.829748
1935.357687	273041.930565	37.834765
1937.199764	273504.690968	37.839783
1939.431976	273963.169337	37.844800
1941.579835	274424.683740	37.849818
1943.137127	274896.735251	37.854836
1945.263789	275344.661155	37.859853
1947.260998	275812.142037	37.864871
1949.274579	276285.563435	37.869888
1951.437667	276731.854946	37.874906
1953.130363	277195.572961	37.879924
1954.981954	277651.820921	37.884941
1957.433215	278122.752912	37.889959
1959.067459	278593.158298	37.894976
1961.209499	279059.541437	37.899994
1962.918646	279538.543519	37.905012
1965.326877	280000.917768	37.910029
1967.607668	280463.083321	37.915047
1969.554176	280927.970108	37.920064
1971.852433	281397.344527	37.925082
1973.799221	281866.496331	37.930100
1975.815330	282319.353041	37.935117
1977.849017	282782.823471	37.940135
1979.748994	283244.257190	37.945152
1981.984679	283695.372048	37.950170
1983.561109	284157.694860	37.955188
1985.867990	284620.962569	37.960205
1987.738007	285077.671351	37.965223
1989.752440	285549.671754	37.970240
1991.567218	286001.128877	37.975258
1993.493030	286472.048767	37.980276
1995.456141	286937.830021	37.985293
1997.465900	287404.084677	37.990311
1999.173729	287877.372821	37.995328
2001.455445	288344.925676	38.000346
2003.140457	288812.905667	38.005364
2005.116954	289293.561487	38.010381
2007.199915	289768.660728	38.015399
2009.008596	290240.196704	38.020416
2011.014233	290711.698434	38.025434
2013.030599	291179.259641	38.030452
2014.692703	291639.460824	38.035469
2016.933957	292095.399098	38.040487
2018.792955	292549.011205	38.045504
2020.869994	292994.076728	38.050522
2022.617476	293461.571961	38.055540
2024.230998	293917.251319	38.060557
2026.364597	294388.793772	38.065575
2028.386132	294862.257714	38.070592
2030.277905	295341.684473	38.075610
2032.191832	295807.364654	38.080628
2034.004934	296282.304691	38.085645
2036.348748	296772.470467	38.090663
2037.935748	297264.867036	38.095680
2040.026794	297748.314000	38.100698
2041.890978	298259.531226	38.105716
2043.565978	298757.646239	38.110733
2046.061510	299255.470942	38.115751
2047.975941	299779.091909	38.120768
2049.864595	300276.732329	38.125786
2052.157457	300800.894925	38.130804
2053.756924	301312.394160	38.135821
2055.834085	301829.754793	38.140839
2057.727153	302352.120858	38.145856
2060.075668	302881.139053	38.150874
2061.977432	303410.202570	38.155892
2063.842686	303951.180179	38.160909
2066.535659	304477.592528	38.165927
2068.309587	305022.667601	38.170944
2070.545265	305561.415536	38.175962
2072.464863	306098.079024	38.180980
2074.531009	306641.114780	38.185997
2076.715634	307183.314829	38.191015
2078.617265	307734.091077	38.196032
2081.176510	308273.682612	38.201050
2083.264862	308827.849136	38.206068
2085.168350	309377.242692	38.211085
2087.711702	309927.364887	38.216103
2089.651608	310483.779254	38.221120
2092.024837	311020.259461	38.226138
2093.667422	311569.401502	38.231156
2095.926348	312127.173534	38.236173
2098.820621	312667.720907	38.241191
2100.674685	313235.226805	38.246208
2102.948027	313777.544692	38.251226
2105.399969	314323.688942	38.256244
2107.359975	314858.914971	38.261261
2109.692698	315392.602705	38.266279
2111.960850	315945.672031	38.271296
2114.111296	316485.704557	38.276314
2116.324762	317025.697144	38.281332
2118.908101	317570.118956	38.286349
2121.043419	318107.627568	38.291367
2123.019515	318644.015604	38.296384
2125.433113	319176.645355	38.301402
2127.449871	319712.104093	38.306420
2129.649330	320236.076823	38.311437
2131.777083	320760.336541	38.316455
2133.919758	321296.853482	38.321472
2136.065540	321822.168119	38.326490
2138.114509	322348.078443	38.331508
2140.149840	322883.711224	38.336525
2142.319558	323407.079213	38.341543
2144.281029	323949.367382	38.346560
2146.575759	324478.367748	38.351578
2148.811145	325020.829851	38.356596
2150.507654	325551.138457	38.361613
2153.403374	326075.963542	38.366631
2154.985896	326603.742848	38.371648
2157.277615	327115.430958	38.376666
2159.681108	327613.919604	38.381684
2161.420843	328118.936839	38.386701
2163.906295	328612.528950	38.391719
2165.807129	329123.451703	38.396736
2167.829208	329633.156707	38.401754
2169.808193	330140.731758	38.406772
2171.898969	330658.108648	38.411789
2173.921400	331161.275427	38.416807
2176.166112	331685.014973	38.421824
2177.920832	332215.481726	38.426842
2180.127445	332727.793842	38.431860
2182.531477	333272.511819	38.436877
2184.493818	333796.328698	38.441895
2186.656464	334344.299764	38.446912
2188.540208	334877.308651	38.451930
2190.767928	335413.733172	38.456948
2192.581395	335978.879923	38.461965
2195.095627	336514.459050	38.466983
2197.351923	337085.892259	38.472000
2199.334094	337634.696662	38.477018
2201.930477	338198.649357	38.482036
2203.941908	338762.540094	38.487053
2206.336679	339321.259314	38.492071
2208.319605	339886.411391	38.497088
2210.719935	340458.722187	38.502106
2212.765759	341029.942722	38.507124
2214.884603	341609.952097	38.512141
2217.276800	342184.249414	38.517159
2219.572393	342757.388370	38.522176
2221.594484	343333.408349	38.527194
2224.090882	343914.647686	38.532212
2226.240664	344502.282237	38.537229
2228.468444	345081.800411	38.542247
2230.439429	345672.241726	38.547264
2232.782383	346265.456678	38.552282
2235.579373	346856.837956	38.557300
2237.577533	347463.494597	38.562317
2239.804485	348036.783639	38.567335
2242.082923	348640.358359	38.572352
2244.486854	349233.880116	38.577370
2246.980750	349833.672771	38.582388
2249.088584	350419.360702	38.587405
2251.456600	351010.809218	38.592423
2253.734102	351614.800652	38.597440
2256.245222	352211.868295	38.602458
2258.563305	352801.626039	38.607476
2260.535729	353403.486058	38.612493
2263.133110	353992.445517	38.617511
2265.198719	354583.869830	38.622528
2267.448707	355185.506658	38.627546
2269.916511	355778.801689	38.632564
2272.261134	356377.284845	38.637581
2274.686087	356985.261070	38.642599
2277.342243	357573.450177	38.647616
2279.303219	358171.158779	38.652634
2281.734339	358752.187724	38.657652
2283.620666	359349.815247	38.662669
2285.840990	359942.837340	38.667687
2288.092458	360541.122690	38.672704
2290.276989	361147.731660	38.677722
2292.723354	361739.269010	38.682740
2294.825764	362356.477730	38.687757
2297.292011	362955.046310	38.692775
2299.486996	363556.390321	38.697792
2301.723058	364164.770694	38.702810
2303.982801	364766.034464	38.707828
2305.929685	365375.331289	38.712845
2308.602970	365950.912063	38.717863
2310.837943	366534.318740	38.722880
2312.761633	367112.592973	38.727898
2314.904600	367693.003593	38.732916
2316.996575	368275.189203	38.737933
2319.513743	368866.832902	38.742951
2321.794986	369461.600580	38.747968
2323.743101	370067.320374	38.752986
2326.053737	370665.056663	38.758004
2327.698184	371269.791997	38.763021
2329.926987	371886.392251	38.768039
2332.407651	372502.559905	38.773056
2334.581116	373140.274972	38.778074
2336.904230	373757.638944	38.783092
2339.233986	374389.345657	38.788109
2341.605252	375020.907352	38.793127
2344.088204	375668.543183	38.798144
2346.424234	376314.872459	38.803162
2348.775685	376944.043966	38.808180
2350.930571	377590.810315	38.813197
2353.599840	378243.413470	38.818215
2355.671474	378900.109318	38.823232
2358.208987	379552.506142	38.828250
2360.522083	380206.524843	38.833268
2362.855500	380866.055163	38.838285
2365.429829	381528.397896	38.843303
2368.176983	382198.356264	38.848320
2370.069587	382865.500807	38.853338
2372.868458	383532.963924	38.858356
2375.055074	384202.948384	38.863373
2377.784242	384864.361325	38.868391
2380.436725	385528.612877	38.873408
2382.410319	386202.926243	38.878426
2385.540465	386869.175341	38.883444
2387.794903	387549.498263	38.888461
2390.338212	388220.378976	38.893479
2392.814023	388875.792717	38.898496
2395.352183	389552.349543	38.903514
2397.837754	390212.854172	38.908532
2400.188884	390885.027293	38.913549
2402.626324	391553.369226	38.918567
2404.995094	392226.777404	38.923584
2407.896697	392891.287291	38.928602
2410.632839	393553.782157	38.933620
2412.771932	394221.759659	38.938637
2415.423160	394878.561800	38.943655
2418.019004	395549.272934	38.948672
2419.875799	396205.720641	38.953690
2422.599597	396864.291614	38.958708
2425.070937	397538.196742	38.963725
2427.346544	398202.817908	38.968743
2429.836007	398861.534597	38.973760
2431.932367	399542.601602	38.978778
2434.300696	400218.742195	38.983796
2436.608315	400894.826177	38.988813
2438.995275	401570.703669	38.993831
2441.757513	402259.172641	38.998848
2443.729130	402931.716108	39.003866
2446.424006	403620.568358	39.008884
2448.668011	404301.724885	39.013901
2450.963226	404994.384422	39.018919
2453.578757	405669.466701	39.023936
2456.185867	406362.724570	39.028954
2458.589852	407042.951125	39.033972
2460.643699	407743.789724	39.038989
2463.393994	408430.283354	39.044007
2465.807131	409113.673958	39.049024
2468.538569	409799.426590	39.054042
2471.112789	410458.108355	39.059060
2473.193643	411117.995170	39.064077
2475.995076	411764.296390	39.069095
2478.324099	412412.584831	39.074112
2480.564853	413074.372217	39.079130
2482.889562	413723.160984	39.084148
2485.471711	414398.890451	39.089165
2487.595498	415047.983351	39.094183
2490.002788	415721.123914	39.099200
2492.324172	416409.684431	39.104218
2494.832975	417082.164846	39.109236
2497.484675	417761.669493	39.114253
2499.697437	418450.800777	39.119271
2502.063016	419140.825069	39.124288
2504.509234	419838.768389	39.129306
2507.259736	420544.719699	39.134324
2509.414933	421241.962988	39.139341
2511.762997	421948.903194	39.144359
2514.231642	422663.171303	39.149376
2516.773184	423393.053653	39.154394
2519.128523	424118.641019	39.159412
2521.697571	424834.196663	39.164429
2524.389093	425567.837628	39.169447
2526.765683	426289.610028	39.174464
2529.194459	427042.995823	39.179482
2531.858663	427783.105238	39.184500
2534.473615	428520.010425	39.189517
2536.649155	429282.176559	39.194535
2539.777756	430023.456026	39.199552
2541.990536	430778.733688	39.204570
2544.927310	431525.920287	39.209588
2547.252452	432282.295279	39.214605
2549.693915	433050.875812	39.219623
2552.470438	433801.862768	39.224640
2555.113106	434574.155679	39.229658
2557.871506	435318.263404	39.234676
2560.639779	436094.634599	39.239693
2562.977700	436858.145217	39.244711
2565.771077	437622.718970	39.249728
2567.966703	438393.792312	39.254746
2570.602884	439160.009849	39.259764
2573.462446	439935.677416	39.264781
2575.557756	440716.048676	39.269799
2578.722464	441493.534403	39.274816
2580.884294	442279.203039	39.279834
2583.507031	443055.154679	39.284852
2586.193394	443840.579763	39.289869
2588.648571	444626.723000	39.294887
2591.242575	445407.553659	39.299904
2593.817190	446202.119029	39.304922
2596.198950	446989.857921	39.309940
2599.020516	447785.993340	39.314957
2601.551012	448588.166303	39.319975
2604.553316	449382.037303	39.324992
2606.914479	450173.404864	39.330010
2609.750900	450964.057426	39.335028
2612.361822	451760.381697	39.340045
2614.431326	452564.603614	39.345063
2617.740999	453355.037154	39.350080
2620.152180	454157.674545	39.355098
2622.664813	454953.488168	39.360116
2625.568775	455752.341419	39.365133
2628.006928	456557.762870	39.370151
2630.914553	457355.288825	39.375168
2633.249155	458162.332365	39.380186
2635.778495	458960.919286	39.385204
2638.615747	459756.087194	39.390221
2640.836640	460562.042312	39.395239
2643.529641	461327.143706	39.400256
2646.301085	462100.543202	39.405274
2648.552604	462868.236042	39.410292
2651.760044	463641.200136	39.415309
2653.673184	464411.314844	39.420327
2656.526930	465189.835980	39.425344
2659.013536	465973.440462	39.430362
2661.803738	466773.033786	39.435380
2664.228018	467551.531248	39.440397
2666.787098	468350.036282	39.445415
2669.714467	469142.889117	39.450432
2672.454984	469938.013702	39.455450
2674.861804	470746.498972	39.460468
2677.861957	471534.541522	39.465485
2680.008256	472356.288845	39.470503
2683.146863	473162.984045	39.475520
2685.370838	473973.685282	39.480538
2687.274571	474795.618515	39.485556
2690.091058	475626.305671	39.490573
2692.873022	476476.963410	39.495591
2695.208816	477305.432135	39.500608
2698.231784	478165.619302	39.505626
2700.873562	479015.728370	39.510644
2703.622571	479870.123281	39.515661
2706.104485	480728.158035	39.520679
2709.230491	481595.387715	39.525696
2711.732861	482459.396523	39.530714
2714.478580	483330.140000	39.535732
2717.484067	484202.060523	39.540749
2719.968625	485078.214721	39.545767
2722.900134	485947.436696	39.550784
2725.983469	486817.146236	39.555802
2728.505933	487701.948065	39.560820
2731.107120	488576.849471	39.565837
2734.076219	489464.567704	39.570855
2736.684243	490351.492727	39.575872
2739.401082	491238.556354	39.580890
2742.354224	492126.242010	39.585908
2745.450032	493007.399064	39.590925
2747.763051	493914.778608	39.595943
2750.630247	494808.243527	39.600960
2753.780411	495695.560218	39.605978
2756.738480	496590.530958	39.610996
2759.682720	497477.031385	39.616013
2762.421179	498381.680089	39.621031
2765.220375	499266.243407	39.626048
2768.009858	500151.013663	39.631066
2770.618299	501053.571775	39.636084
2773.811153	501948.116226	39.641101
2776.465801	502845.071339	39.646119
2779.530213	503743.019415	39.651136
2782.247049	504625.897523	39.656154
2784.943186	505524.161494	39.661172
2787.824334	506414.075983	39.666189
2790.504759	507307.604915	39.671207
2793.378349	508203.472531	39.676224
2796.509468	509098.592357	39.681242
2799.301237	509999.868323	39.686260
2802.209553	510875.365715	39.691277
2805.095448	511766.595651	39.696295
2808.100321	512657.251789	39.701312
2810.838870	513535.855924	39.706330
2813.572662	514427.918270	39.711348
2816.362172	515307.523581	39.716365
2818.960818	516209.333558	39.721383
2821.992880	517096.255872	39.726400
2824.998798	517983.786766	39.731418
2827.459317	518858.559321	39.736436
2830.605452	519708.583548	39.741453
2832.952101	520565.543852	39.746471
2835.841782	521412.442767	39.751488
2838.980608	522254.518563	39.756506
2841.520606	523105.007679	39.761524
2844.540728	523941.972410	39.766541
2847.043358	524806.071555	39.771559
2849.824516	525659.297965	39.776576
2852.645582	526514.785661	39.781594
2855.660452	527380.364042	39.786612
2857.946776	528241.279168	39.791629
2860.946387	529115.872637	39.796647
2863.780588	529986.867092	39.801664
2866.771454	530869.061025	39.806682
2869.472984	531755.578898	39.811700
2872.227942	532638.812716	39.816717
2874.569967	533549.190986	39.821735
2877.521776	534443.205284	39.826752
2880.437996	535347.739027	39.831770
2883.215148	536258.881827	39.836788
2886.513280	537162.483833	39.841805
2889.205213	538088.822182	39.846823
2892.133390	539010.684170	39.851840
2894.998194	539938.081482	39.856858
2897.766622	540879.620914	39.861876
2900.804028	541798.114434	39.866893
2903.581589	542742.395500	39.871911
2906.479423	543681.161086	39.876928
2909.602941	544630.036274	39.881946
2912.147622	545583.921175	39.886964
2915.721653	546525.451578	39.891981
2918.335154	547485.480364	39.896999
2921.211249	548442.080571	39.902016
2924.273073	549395.164791	39.907034
2927.529891	550349.055522	39.912052
2930.504481	551302.524026	39.917069
2933.595394	552277.772527	39.922087
2936.480600	553233.080733	39.927104
2939.710263	554187.963094	39.932122
2942.704798	555147.992912	39.937140
2945.227315	556112.403883	39.942157
2948.661763	557082.574582	39.947175
2951.517347	558045.585138	39.952192
2954.524568	559022.518244	39.957210
2957.665981	559988.505874	39.962228
2960.523546	560949.295544	39.967245
2963.273685	561927.111049	39.972263
2966.165799	562902.971869	39.977280
2969.028995	563874.997901	39.982298
2972.053079	564865.957839	39.987316
2975.412500	565839.412433	39.992333
2978.409305	566815.564984	39.997351
2981.316113	567805.716573	40.002368
2984.533876	568777.968536	40.007386
2987.164764	569747.683278	40.012404
2990.383639	570736.653266	40.017421
2993.265905	571711.598306	40.022439
2996.439163	572700.222177	40.027456
2999.304122	573682.747264	40.032474
3002.200727	574670.208549	40.037492
3005.515759	575652.104146	40.042509
3008.282461	576644.097775	40.047527
3011.116326	577631.887644	40.052544
3014.694885	578615.914583	40.057562
3017.417057	579600.456024	40.062580
3020.322574	580591.258644	40.067597
3023.535876	581582.883688	40.072615
3026.463065	582564.446107	40.077632
3029.585269	583510.896807	40.082650
3032.244028	584462.013538	40.087668
3035.503065	585403.130106	40.092685
3038.320070	586339.684386	40.097703
3041.292108	587290.828286	40.102720
3044.561045	588234.329397	40.107738
3046.895611	589192.746237	40.112756
3049.738547	590152.606295	40.117773
3053.041649	591119.880340	40.122791
3055.973459	592091.847186	40.127808
3059.457819	593056.077489	40.132826
3062.094692	594036.551360	40.137844
3064.850174	595007.856700	40.142861
3067.885840	595999.172638	40.147879
3071.001373	596993.246539	40.152896
3074.268434	597990.716699	40.157914
3077.299885	598978.825482	40.162932
3080.129294	599985.511370	40.167949
3082.886898	601005.039732	40.172967
3085.791255	602026.907024	40.177984
3089.212116	603049.649634	40.183002
3092.131470	604084.597596	40.188020
3094.973634	605118.763786	40.193037
3098.297087	606151.455464	40.198055
3101.064030	607204.062232	40.203072
3104.276752	608253.595340	40.208090
3107.456848	609315.294506	40.213108
3110.737197	610369.872758	40.218125
3113.998099	611420.553084	40.223143
3116.625705	612500.450593	40.228160
3120.221536	613557.226879	40.233178
3123.214274	614642.307738	40.238196
3126.133079	615711.092623	40.243213
3129.468905	616803.905370	40.248231
3132.630699	617879.289710	40.253248
3135.839246	618966.208562	40.258266
3139.191165	620061.992966	40.263284
3142.492728	621143.480872	40.268301
3145.759138	622237.710450	40.273319
3148.907519	623330.749397	40.278336
3152.168990	624414.165430	40.283354
3155.177366	625512.751815	40.288372
3158.581149	626596.373587	40.293389
3162.003723	627704.008134	40.298407
3164.650703	628812.953786	40.303424
3168.201740	629894.966702	40.308442
3171.331062	631001.755842	40.313460
3174.728876	632100.895095	40.318477
3178.015833	633200.636543	40.323495
3180.903155	634299.130312	40.328512
3184.364401	635384.486268	40.333530
3187.747902	636502.232115	40.338548
3191.194323	637602.181514	40.343565
3194.251038	638699.134167	40.348583
3197.626359	639802.004417	40.353600
3200.918114	640891.749564	40.358618
3203.881646	641997.843921	40.363636
3207.213595	643093.932128	40.368653
3210.558017	644200.522728	40.373671
3213.445652	645294.751195	40.378688
3216.904813	646385.177183	40.383706
3219.821524	647494.120576	40.388724
3223.043060	648600.000173	40.393741
3226.490648	649690.767415	40.398759
3229.414554	650805.075320	40.403776
3232.978351	651898.622112	40.408794
3235.839209	653005.219027	40.413812
3239.172191	654102.248013	40.418829
3242.605394	655162.075422	40.423847
3245.534648	656216.442379	40.428864
3248.645264	657273.654487	40.433882
3251.895540	658338.996144	40.438900
3254.863631	659396.002077	40.443917
3258.685672	660444.835929	40.448935
3261.381850	661531.726897	40.453952
3264.726781	662591.757526	40.458970
3267.928312	663669.712956	40.463988
3270.803633	664752.627771	40.469005
3274.221033	665831.748112	40.474023
3277.285241	666928.716891	40.479040
3280.637704	668016.656421	40.484058
3283.926620	669120.947210	40.489076
3286.318746	670227.047686	40.494093
3289.647061	671343.457411	40.499111
3292.776381	672472.497604	40.504128
3296.199673	673603.093826	40.509146
3299.545488	674730.135983	40.514164
3302.359915	675878.703117	40.519181
3305.886198	677031.335287	40.524199
3308.894597	678193.799123	40.529216
3312.379872	679351.864341	40.534234
3315.770054	680519.388709	40.539252
3318.459853	681704.664646	40.544269
3322.153898	682885.648158	40.549287
3325.034386	684079.078803	40.554304
3328.556785	685271.055521	40.559322
3331.826048	686478.210015	40.564340
3334.968991	687686.117945	40.569357
3338.853592	688890.614782	40.574375
3342.095471	690120.765128	40.579392
3345.518536	691327.194977	40.584410
3349.053080	692543.912939	40.589428
3352.374626	693765.411337	40.594445
3355.663851	694981.637905	40.599463
3359.442781	696219.836220	40.604480
3362.325274	697445.363126	40.609498
3366.022002	698684.666818	40.614516
3369.059369	699921.921051	40.619533
3372.648997	701155.439413	40.624551
3375.774439	702400.804193	40.629568
3379.960192	703636.945463	40.634586
3383.433948	704874.860937	40.639604
3386.561424	706135.444766	40.644621
3390.116768	707371.799356	40.649639
3393.357619	708612.930787	40.654656
3397.039150	709855.394192	40.659674
3400.312339	711112.597470	40.664692
3403.619127	712368.520252	40.669709
3407.497624	713614.560306	40.674727
3410.839926	714869.710101	40.679744
3413.897674	716123.284811	40.684762
3417.231553	717375.489008	40.689780
3420.870142	718638.091279	40.694797
3424.454844	719881.518727	40.699815
3427.900190	721154.158285	40.704832
3430.798991	722407.161854	40.709850
3434.495209	723667.704807	40.714868
3438.088897	724922.832345	40.719885
3441.696646	726186.118327	40.724903
3445.057697	727456.860110	40.729920
3448.656308	728711.801839	40.734938
3452.288556	729970.002643	40.739956
3455.523227	731239.779890	40.744973
3458.814900	732495.965498	40.749991
3462.293217	733750.641066	40.755008
3465.899578	734989.916277	40.760013
3469.323797	736193.924421	40.765018
3472.411649	737339.024010	40.770023
3475.787848	738411.234796	40.775028
3478.853889	739438.040026	40.780032
3481.815191	740390.735413	40.785037
3485.041335	741271.858210	40.790042
3487.473608	742088.430783	40.795047
3490.354044	742840.515589	40.800052
3493.043217	743530.312851	40.805056
3495.402157	744150.792106	40.810061
3497.910897	744707.377851	40.815066
3499.817310	745209.945545	40.820071
3502.583971	745647.340841	40.825076
3504.387431	746021.753271	40.830080
3506.311666	746330.492635	40.835085
3508.011120	746605.105893	40.840090
3509.426040	746821.439555	40.845095
3511.188407	746992.935462	40.850100
3512.606983	747123.070976	40.855104
3513.993694	747202.506050	40.860109
3515.630498	747236.285894	40.865114
3516.679913	747250.790352	40.870119
3517.908563	747213.622866	40.875124
3518.631075	747147.430785	40.880128
3519.496761	747049.240039	40.885133
3520.696985	746918.919050	40.890138
3520.960235	746760.184654	40.895143
3521.849038	746582.217396	40.900148
3522.224864	746385.895502	40.905152
3522.926997	746168.608031	40.910157
3523.564757	745922.410465	40.915162
3524.191379	745675.119569	40.920167
3524.912223	745395.181475	40.925172
3525.146715	745111.754419	40.930176
3525.456959	744801.116010	40.935181
3525.613888	744487.524411	40.940186
3525.993958	744166.171204	40.945191
3526.250509	743815.012852	40.950196
3526.506643	743467.102084	40.955200
3526.939384	743114.301273	40.960205
3527.248110	742734.408220	40.965210
3527.225697	742363.847892	40.970215
3527.303249	741974.808225	40.975220
3527.440963	741591.327795	40.980224
3527.395726	741191.637158	40.985229
3527.697266	740781.136557	40.990234
3527.379771	740381.944484	40.995239
3527.604769	739970.771511	41.000244
3527.396279	739555.740783	41.005248
3527.423828	739149.999181	41.010253
3527.799660	738723.648636	41.015258
3527.233824	738318.457105	41.020263
3527.526200	737886.880682	41.025268
3527.272156	737474.222743	41.030272
3527.281392	737042.647305	41.035277
3527.337787	736628.162606	41.040282
3527.219800	736205.074322	41.045287
3527.177075	735781.654334	41.050292
3527.430324	735354.797692	41.055296
3526.947064	734918.932521	41.060301
3527.024119	734492.752002	41.065306
3527.082355	734074.175108	41.070311
3526.725334	733629.358559	41.075316
3526.589719	733214.036111	41.080320
3526.242608	732779.369240	41.085325
3526.474049	732355.822696	41.090330
3526.075653	731943.646890	41.095335
3526.273088	731517.388276	41.100340
3526.377123	731096.074513	41.105344
3525.805854	730674.652032	41.110349
3525.765754	730251.188686	41.115354
3525.257484	729829.068093	41.120359
3525.279342	729405.500930	41.125364
3525.206619	728998.470936	41.130368
3524.772433	728594.798954	41.135373
3524.836985	728179.730427	41.140378
3524.578864	727775.245818	41.145383
3524.490480	727369.078333	41.150388
3524.262782	726976.984151	41.155392
3524.426239	726561.371238	41.160397
3524.235806	726167.052083	41.165402
3524.023162	725771.429290	41.170407
3523.930343	725376.560543	41.175412
3523.826492	724983.706435	41.180416
3523.451087	724581.164842	41.185421
3523.664610	724201.106278	41.190426
3523.072892	723801.238484	41.195431
3523.318049	723411.473476	41.200436
3523.049531	723041.056595	41.205440
3522.973930	722654.084494	41.210445
3522.622671	722277.698625	41.215450
3522.133968	721904.391910	41.220455
3521.863617	721527.611591	41.225460
3522.073834	721154.850030	41.230464
3521.985030	720779.394033	41.235469
3521.859618	720415.628809	41.240474
3521.490966	720050.251425	41.245479
3521.347566	719692.506991	41.250484
3521.537928	719334.146709	41.255488
3521.259855	718980.509865	41.260493
3521.258151	718609.652914	41.265498
3521.167691	718262.848349	41.270503
3520.884586	717904.752713	41.275508
3520.404617	717564.629555	41.280512
3520.387472	717209.981997	41.285517
3520.472603	716862.743271	41.290522
3520.033599	716521.975787	41.295527
3520.009832	716176.710881	41.300532
3519.529779	715849.466012	41.305536
3519.565640	715526.241229	41.310541
3519.704231	715171.184242	41.315546
3519.179104	714857.353748	41.320551
3519.050589	714520.522555	41.325556
3519.282878	714208.081264	41.330560
3519.092674	713886.964546	41.335565
3519.088336	713558.659142	41.340570
3518.702299	713239.584684	41.345575
3518.157708	712918.340697	41.350580
3518.613336	712601.386379	41.355584
3518.131632	712298.223315	41.360589
3518.315492	711987.941463	41.365594
3517.742664	711679.758359	41.370599
3517.737164	711372.165504	41.375604
3517.788423	711071.352660	41.380608
3517.442075	710773.175995	41.385613
3517.276219	710480.519054	41.390618
3517.224325	710187.684353	41.395623
3517.055539	709893.915595	41.400628
3517.060108	709605.370755	41.405632
3516.426006	709315.233345	41.410637
3516.374662	709029.408947	41.415642
3516.342437	708750.225229	41.420647
3516.206555	708471.943251	41.425652
3516.332120	708202.944344	41.430656
3515.789690	707917.660301	41.435661
3515.658561	707650.474004	41.440666
3515.375467	707395.967718	41.445671
3515.808009	707119.534588	41.450676
3515.474956	706859.706862	41.455680
3515.514738	706591.317211	41.460685
3515.362226	706326.477169	41.465690
3515.263368	706066.586901	41.470695
3515.021969	705813.268600	41.475700
3515.175484	705549.943672	41.480704
3514.778784	705295.741687	41.485709
3515.017553	705039.142523	41.490714
3514.693071	704791.818418	41.495719
3514.392536	704528.139751	41.500724
3514.351211	704290.193157	41.505728
3513.898671	704052.655535	41.510733
3513.881445	703804.656424	41.515738
3513.855791	703566.488640	41.520743
3513.867858	703332.580864	41.525748
3513.786706	703091.279127	41.530752
3513.653426	702858.724016	41.535757
3513.646795	702642.041746	41.540762
3513.386994	702415.309020	41.545767
3513.154271	702164.863828	41.550772
3513.204062	701950.242002	41.555776
3512.918702	701730.551789	41.560781
3513.094747	701505.611856	41.565786
3513.145365	701291.371212	41.570791
3512.698455	701063.938393	41.575796
3512.719430	700841.690487	41.580800
3512.364391	700646.236791	41.585805
3512.380626	700425.619131	41.590810
3512.185052	700218.201599	41.595815
3512.137072	700002.106629	41.600820
3512.063133	699808.029235	41.605824
3511.655087	699608.286570	41.610829
3511.914456	699402.464690	41.615834
3511.645359	699204.529032	41.620839
3511.495829	698993.993081	41.625844
3510.993806	698815.125163	41.630848
3511.123513	698625.113863	41.635853
3511.263480	698433.605426	41.640858
3510.872779	698243.522488	41.645863
3510.825520	698060.636991	41.650868
3511.007479	697888.149925	41.655872
3510.893927	697700.196997	41.660877
3511.102647	697509.701131	41.665882
3510.646378	697335.667761	41.670887
3510.588587	697148.489345	41.675892
3510.699284	696978.134089	41.680896
3510.127187	696790.137859	41.685901
3510.466673	696611.881990	41.690906
3510.130480	696450.937823	41.695911
3509.861097	696275.659391	41.700916
3509.898973	696107.188809	41.705920
3509.827915	695948.280212	41.710925
3509.859267	695773.688144	41.715930
3509.913937	695612.763752	41.720935
3509.816224	695452.756647	41.725940
3509.898465	695291.871605	41.730944
3509.552365	695122.749339	41.735949
3509.948543	694955.938340	41.740954
3509.397254	694804.697149	41.745959
3509.730953	694635.204903	41.750964
3509.426312	694485.260398	41.755968
3509.453106	694332.274688	41.760973
3509.426247	694162.584156	41.765978
3509.360540	694023.335281	41.770983
3508.941586	693866.933480	41.775988
3509.059419	693715.165561	41.780992
3509.085171	693566.046370	41.785997
3509.024008	693403.907264	41.791002
3508.749784	693258.513068	41.796007
3508.839342	693113.653445	41.801012
3508.754952	692969.068839	41.806016
3508.753328	692822.229825	41.811021
3508.696562	692671.069786	41.816026
3508.539587	692529.972065	41.821031
3508.515933	692384.174096	41.826036
3508.646008	692249.789984	41.831040
3508.197677	692118.633198	41.836045
3508.281786	691975.497114	41.841050
3508.242504	691842.925692	41.846055
3508.360735	691707.540408	41.851060
3508.215971	691579.957359	41.856064
3507.928538	691432.694829	41.861069
3507.975451	691299.205630	41.866074
3507.907154	691172.051921	41.871079
3507.784986	691047.144150	41.876084
3508.148577	690916.631973	41.881088
3507.961381	690789.641684	41.886093
3508.169917	690649.399364	41.891098
3507.528256	690534.172717	41.896103
3507.538638	690405.402982	41.901108
3507.845309	690279.468475	41.906112
3507.386473	690158.683856	41.911117
3507.541998	690037.348551	41.916122
3507.695982	689923.575210	41.921127
3507.808648	689783.882504	41.926132
3507.597991	689663.697201	41.931136
3507.461363	689546.981358	41.936141
3507.600226	689413.001076	41.941146
3507.415420	689283.700036	41.946151
3507.462056	689180.683652	41.951156
3507.511631	689052.634506	41.956160
3507.354109	688935.565822	41.961165
3507.263437	688812.263975	41.966170
3507.078695	688699.526261	41.971175
3506.788479	688580.334899	41.976180
3507.141656	688467.555409	41.981184
3506.759522	688365.794758	41.986189
3507.090417	688254.111155	41.991194
3506.997877	688153.892971	41.996199
3506.738602	688040.412761	42.001204
3506.699963	687926.795226	42.006208
3506.563836	687825.983341	42.011213
3506.551892	687718.629862	42.016218
3506.566757	687619.980722	42.021223
3506.365657	687515.045027	42.026228
3506.361730	687403.057663	42.031232
3506.085375	687309.579715	42.036237
3506.173150	687207.927663	42.041242
3506.354684	687114.471794	42.046247
3506.377065	687012.927874	42.051252
3506.055949	686916.715617	42.056256
3505.777331	686821.441076	42.061261
3505.998499	686726.730272	42.066266
3505.767739	686635.378230	42.071271
3505.575018	686547.802087	42.076276
3506.013903	686450.513867	42.081280
3506.135459	686368.558899	42.086285
3506.053836	686263.887670	42.091290
3505.810585	686176.764278	42.096295
3505.950782	686091.717403	42.101300
3505.891131	685986.093525	42.106304
3505.736766	685896.911792	42.111309
3505.804404	685806.497843	42.116314
3505.631702	685715.375865	42.121319
3505.716653	685621.920517	42.126324
3505.532360	685541.501951	42.131328
3505.241766	685462.743042	42.136333
3505.778478	685373.691209	42.141338
3505.761047	685279.552234	42.146343
3505.423470	685206.324915	42.151348
3505.707920	685119.602264	42.156352
3505.071092	685037.262388	42.161357
3505.669275	684954.369755	42.166362
3505.489912	684873.994253	42.171367
3505.304532	684788.690106	42.176372
3505.552182	684696.642261	42.181376
3505.147688	684623.222120	42.186381
3505.340291	684533.571523	42.191386
3505.086881	684456.291420	42.196391
3505.105624	684377.571712	42.201396
3505.054683	684296.970793	42.206400
3505.061836	684234.831760	42.211405
3505.187406	684145.487131	42.216410
3504.964100	684067.999609	42.221415
3504.837391	683994.080498	42.226420
3505.073359	683919.403939	42.231424
3504.864914	683844.551038	42.236429
3505.063488	683767.738330	42.241434
3504.699789	683700.777077	42.246439
3504.560045	683629.297017	42.251444
3504.911361	683556.888984	42.256448
3504.977906	683480.543760	42.261453
3505.403556	683407.873327	42.266458
3504.965571	683343.062860	42.271463
3504.880639	683268.234672	42.276468
3504.906228	683193.188476	42.281472
3504.638910	683120.978519	42.286477
3504.721402	683048.560959	42.291482
3504.773217	682985.061547	42.296487
3504.595596	682905.315756	42.301492
3504.873314	682841.529135	42.306496
3504.428268	682771.088620	42.311501
3504.844546	682697.916108	42.316506
3504.187694	682635.477214	42.321511
3504.288483	682577.145982	42.326516
3504.721831	682504.566703	42.331520
3504.287330	682441.342849	42.336525
3504.343459	682377.838510	42.341530
3504.676508	682314.487303	42.346535
3504.585246	682253.496421	42.351540
3504.547087	682175.414518	42.356544
3504.439953	682130.959485	42.361549
3504.562722	682053.696655	42.366554
3504.701903	681986.191750	42.371559
3504.606496	681927.888714	42.376564
3504.441320	681853.460597	42.381568
3504.538546	681794.975563	42.386573
3504.495788	681726.801480	42.391578
3504.280036	681673.148409	42.396583
3504.170125	681607.424906	42.401588
3504.208042	681545.710764	42.406592
3503.973134	681486.132979	42.411597
3504.253407	681424.676918	42.416602
3504.335265	681366.938770	42.421607
3504.091643	681308.805637	42.426612
3504.216311	681248.918030	42.431616
3504.122868	681185.679113	42.436621
3504.210788	681120.716434	42.441626
3504.276454	681073.139755	42.446631
3504.506921	681013.980294	42.451636
3504.263804	680951.162887	42.456640
3504.016062	680908.418570	42.461645
3504.264739	680829.182162	42.466650
3503.897409	680775.897482	42.471655
3503.881494	680728.133224	42.476660
3503.997357	680665.254710	42.481664
3503.945187	680611.668097	42.486669
3504.247049	680548.857757	42.491674
3504.127665	680507.285868	42.496679
3504.210034	680448.446036	42.501684
3504.155950	680373.589130	42.506688
3503.946960	680329.291586	42.511693
3503.937870	680265.633948	42.516698
3504.306240	680214.416501	42.521703
3503.784517	680162.498630	42.526708
3504.313062	680096.908178	42.531712
3503.814293	680050.714349	42.536717
3504.220943	679991.469471	42.541722
3504.047294	679940.987391	42.546727
3504.387996	679874.529668	42.551732
3504.411351	679814.300721	42.556736
3504.087541	679763.344269	42.561741
3503.895135	679704.046815	42.566746
3503.821523	679655.838168	42.571751
3504.211879	679583.392357	42.576756
3504.131299	679534.636255	42.581760
3504.075311	679482.587987	42.586765
3504.016655	679419.231566	42.591770
3504.273863	679360.057077	42.596775
3504.216196	679306.961946	42.601780
3504.475691	679241.708654	42.606784
3504.166224	679195.479340	42.611789
3504.040754	679121.321470	42.616794
3504.093575	679076.875127	42.621799
3503.940116	679029.772365	42.626804
3504.361152	678962.447926	42.631808
3503.983220	678909.552739	42.636813
3504.125573	678848.998968	42.641818
3504.036934	678797.101675	42.646823
3503.901147	678734.002359	42.651828
3504.261514	678671.717622	42.656832
3503.858398	678625.949269	42.661837
3504.122698	678562.234827	42.666842
3504.124835	678505.737410	42.671847
3503.725050	678453.291601	42.676852
3504.069993	678411.434463	42.681856
3503.925292	678361.188078	42.686861
3504.342385	678299.838110	42.691866
3504.355523	678252.803581	42.696871
3503.562673	678190.008113	42.701876
3503.741852	678136.368999	42.706880
3503.877773	678078.700994	42.711885
3503.822629	678030.929236	42.716890
3504.012435	677973.600464	42.721895
3503.768710	677914.648746	42.726900
3503.697989	677863.042205	42.731904
3503.719266	677829.805622	42.736909
3503.798832	677763.126629	42.741914
3503.892219	677712.090108	42.746919
3503.852387	677664.961670	42.751924
3503.860795	677619.867911	42.756928
3503.474174	677568.710393	42.761933
3503.758038	677515.199913	42.766938
3503.635859	677472.967072	42.771943
3503.716018	677431.846720	42.776948
3503.908516	677363.252815	42.781952
3503.684037	677322.829934	42.786957
3503.883421	677257.522735	42.791962
3504.085435	677220.566916	42.796967
3503.600337	677163.792804	42.801972
3503.960537	677097.511240	42.806977
3503.430792	677061.024167	42.811981
3504.234095	677008.969876	42.816986
3504.037832	676957.478641	42.821991
3504.027815	676897.186371	42.826996
3503.730360	676843.867473	42.832001
3503.903521	676795.752749	42.837005
3503.862184	676745.679893	42.842010
3503.883921	676702.273723	42.847015
3503.603105	676643.668851	42.852020
3503.729610	676597.653703	42.857025
3503.681999	676546.634009	42.862029
3503.989967	676484.692047	42.867034
3503.439790	676453.687482	42.872039
3503.668827	676390.811088	42.877044
3503.826468	676330.936011	42.882049
3503.547795	676305.666831	42.887053
3503.388997	676238.567670	42.892058
3503.757502	676201.181698	42.897063
3503.829218	676147.050463	42.902068
3504.183885	676087.191187	42.907073
3503.825800	676051.917713	42.912077
3503.660760	675998.522310	42.917082
3503.840761	675948.209348	42.922087
3503.634457	675903.441648	42.927092
3503.871903	675849.381044	42.932097
3503.544202	675807.922032	42.937101
3503.759453	675755.808136	42.942106
3503.553443	675701.122041	42.947111
3503.522586	675650.194344	42.952116
3503.732151	675601.469409	42.957121
3503.566646	675565.763664	42.962125
3503.343685	675513.571112	42.967130
3503.678207	675478.679709	42.972135
3503.339045	675430.742027	42.977140
3503.662500	675388.775148	42.982145
3503.234106	675345.386986	42.987149
3503.440179	675291.826701	42.992154
3503.411371	675257.393050	42.997159
3503.162495	675212.130654	43.002164
3503.868795	675156.792643	43.007169
3503.380112	675115.257395	43.012173
3503.318589	675075.844518	43.017178
3503.406097	675027.834456	43.022183
3503.363924	674987.520900	43.027188
3503.690618	674940.318257	43.032193
3503.244320	674903.808958	43.037197
3503.855171	674859.499677	43.042202
3503.151466	674798.510671	43.047207
3503.120678	674765.770130	43.052212
3503.681109	674720.770722	43.057217
3503.244534	674688.146617	43.062221
3502.892032	674641.154065	43.067226
3503.471389	674606.019693	43.072231
3502.973462	674553.667709	43.077236
3503.211702	674513.754482	43.082241
3502.977299	674470.081066	43.087245
3503.005511	674429.603974	43.092250
3503.178530	674393.788116	43.097255
3503.172994	674359.696222	43.102260
3503.039302	674311.718931	43.107265
3502.953269	674290.499723	43.112269
3502.728513	674251.808079	43.117274
3502.821190	674223.730634	43.122279
3502.941796	674189.916400	43.127284
3503.162542	674159.524817	43.132289
3502.593369	674122.035815	43.137293
3502.859820	674091.636480	43.142298
3503.090102	674052.021665	43.147303
3502.784412	674019.024736	43.152308
3503.188344	673981.524356	43.157313
3503.341647	673939.977778	43.162317
3503.311688	673894.224308	43.167322
3503.411607	673868.238134	43.172327
3502.970227	673823.299803	43.177332
3503.204592	673778.150212	43.182337
3502.764855	673754.894517	43.187341
3503.074905	673699.264262	43.192346
3503.295778	673670.964648	43.197351
3503.149660	673640.183209	43.202356
3503.359341	673587.360279	43.207361
3503.371221	673559.543394	43.212365
3503.281244	673520.128647	43.217370
3502.827508	673474.642350	43.222375
3502.805997	673445.484728	43.227380
3503.202625	673419.049629	43.232385
3503.017242	673380.148499	43.237389
3503.371965	673338.815309	43.242394
3502.936035	673295.418860	43.247399
3502.971514	673270.388781	43.252404
3503.336540	673223.569964	43.257409
3502.986213	673182.103016	43.262413
3503.094592	673134.478600	43.267418
3503.522137	673089.941915	43.272423
3502.771678	673063.545284	43.277428
3502.948152	673028.371694	43.282433
3502.898740	672997.721760	43.287437
3502.865005	672952.462822	43.292442
3503.388763	672921.867746	43.297447
3502.651218	672897.462563	43.302452
3503.284244	672850.248765	43.307457
3502.959000	672812.913724	43.312461
3502.898277	672785.355766	43.317466
3503.180026	672737.002840	43.322471
3502.784401	672722.361717	43.327476
3503.074891	672683.628543	43.332481
3503.073533	672648.432981	43.337485
3503.143983	672612.876486	43.342490
3502.943922	672570.085897	43.347495
3502.855869	672545.722330	43.352500
3502.853666	672494.822586	43.357505
3502.959162	672462.998752	43.362509
3502.951568	672433.985254	43.367514
3503.329031	672405.556317	43.372519
3502.976813	672350.625450	43.377524
3503.086911	672323.586384	43.382529
3503.216039	672291.558659	43.387533
3503.253402	672246.035329	43.392538
3502.923280	672204.660439	43.397543
3502.966684	672175.787306	43.402548
3502.868158	672133.975101	43.407553
3502.910397	672094.781857	43.412557
3502.878715	672060.785624	43.417562
3503.102650	672027.843977	43.422567
3502.852676	672011.033938	43.427572
3503.287184	671965.742945	43.432577
3503.025260	671924.904004	43.437581
3503.125929	671876.875635	43.442586
3503.388751	671839.888531	43.447591
3503.123327	671814.804444	43.452596
3503.101219	671772.180327	43.457601
3503.119764	671743.409678	43.462605
3503.323063	671699.601369	43.467610
3503.479326	671664.675299	43.472615
3503.205257	671622.640459	43.477620
3503.239627	671572.178418	43.482625
3503.117127	671534.356161	43.487629
3503.308047	671505.057795	43.492634
3503.060150	671453.744177	43.497639
3503.209057	671420.164603	43.502644
3503.224689	671372.945423	43.507649
3503.284716	671345.014331	43.512653
3503.206180	671300.353138	43.517658
3503.287051	671255.864905	43.522663
3503.049898	671213.423275	43.527668
3503.332264	671168.053803	43.532673
3503.258309	671140.293763	43.537677
3503.214173	671096.423705	43.542682
3503.239085	671060.619547	43.547687
3502.832572	671030.470795	43.552692
3503.127353	670974.128886	43.557697
3502.979883	670949.970424	43.562701
3503.176292	670913.987866	43.567706
3503.207212	670878.880093	43.572711
3502.920683	670835.148485	43.577716
3502.728946	670797.384541	43.582721
3503.041001	670762.230009	43.587725
3502.970776	670730.778319	43.592730
3503.034714	670698.556473	43.597735
3503.033294	670666.395150	43.602740
3502.910538	670626.674496	43.607745
3502.683970	670591.059587	43.612749
3502.846165	670564.455663	43.617754
3503.213520	670524.554090	43.622759
3502.558764	670491.652145	43.627764
3502.610645	670456.140435	43.632769
3502.944913	670428.809676	43.637773
3502.592090	670396.356288	43.642778
3502.971414	670361.837422	43.647783
3502.874588	670336.721615	43.652788
3502.741568	670306.675074	43.657793
3502.795697	670269.716209	43.662797
3502.597609	670237.984756	43.667802
3502.792299	670199.705957	43.672807
3502.523831	670184.790592	43.677812
3502.790267	670150.489020	43.682817
3503.138177	670121.758885	43.687821
3502.688969	670086.079025	43.692826
3503.311211	670047.031030	43.697831
3502.890193	670020.571546	43.702836
3502.896468	669984.915982	43.707841
3503.038151	669948.888902	43.712845
3502.784275	669923.947478	43.717850
3503.152972	669880.053609	43.722855
3502.875941	669847.735447	43.727860
3502.877672	669815.371240	43.732865
3502.877865	669790.237993	43.737869
3502.950521	669743.499947	43.742874
3502.885906	669715.634445	43.747879
3502.901946	669685.760841	43.752884
3502.928973	669650.998227	43.757889
3502.718739	669621.012099	43.762893
3502.621057	669570.411517	43.767898
3502.948220	669541.433698	43.772903
3502.889154	669515.611321	43.777908
3502.947879	669472.015986	43.782913
3503.042231	669448.910962	43.787917
3503.147509	669412.189668	43.792922
3503.219957	669366.746409	43.797927
3503.002115	669337.508685	43.802932
3503.035952	669294.714557	43.807937
3502.945861	669262.662813	43.812941
3502.972694	669235.379274	43.817946
3503.202536	669201.977970	43.822951
3502.729381	669162.408647	43.827956
3503.197082	669127.571498	43.832961
3503.306961	669092.045114	43.837965
3503.112797	669058.613432	43.842970
3503.439245	669005.895212	43.847975
3503.180315	668974.568522	43.852980
3503.368093	668933.044066	43.857985
3503.284009	668895.155041	43.862989
3503.223550	668852.174964	43.867994
3503.455468	668812.687486	43.872999
3503.018292	668774.457179	43.878004
3503.271876	668729.579496	43.883009
3503.319721	668692.017033	43.888013
3503.164528	668661.270694	43.893018
3503.168659	668613.840141	43.898023
3503.090199	668566.123715	43.903028
3503.028241	668531.621032	43.908033
3502.965190	668490.933964	43.913037
3502.977244	668462.852647	43.918042
3503.266026	668432.581030	43.923047
3502.912853	668388.250591	43.928052
3503.018664	668351.375480	43.933057
3503.239205	668321.613507	43.938061
3503.040478	668270.274506	43.943066
3503.237584	668243.359064	43.948071
3503.001985	668210.978613	43.953076
3503.247884	668167.944957	43.958081
3502.987202	668137.314056	43.963085
3502.928879	668089.791425	43.968090
3503.241553	668051.733901	43.973095
3503.229969	668015.375600	43.978100
3503.108174	667973.548826	43.983105
3503.255595	667936.665250	43.988109
3503.006465	667904.535371	43.993114
3503.131558	667859.674757	43.998119
3502.888909	667836.671221	44.003124
3503.043934	667794.798045	44.008129
3503.193111	667760.806432	44.013133
3502.684382	667726.474203	44.018138
3503.016415	667685.868222	44.023143
3503.016886	667659.332682	44.028148
3502.768782	667626.303874	44.033153
3502.836833	667599.607394	44.038157
3502.885786	667564.284856	44.043162
3502.866151	667526.080474	44.048167
3502.744856	667501.459983	44.053172
3502.856680	667459.392932	44.058177
3503.149366	667433.656570	44.063181
3502.885313	667394.743736	44.068186
3503.265324	667354.278078	44.073191
3503.043611	667325.683240	44.078196
3503.162639	667281.519230	44.083201
3503.174217	667240.116182	44.088205
3503.150421	667205.602400	44.093210
3503.120024	667164.106176	44.098215
3503.297570	667138.737162	44.103220
3503.405313	667082.602496	44.108225
3503.132631	667042.392714	44.113229
3502.984901	667007.200286	44.118234
3503.096447	666976.005484	44.123239
3503.174920	666940.376475	44.128244
3503.201403	666891.087993	44.133249
3503.267630	666860.947824	44.138253
3503.010910	666825.623036	44.143258
3503.138162	666780.756987	44.148263
3503.025561	666756.681857	44.153268
3503.195667	666718.742275	44.158273
3502.881303	666683.875414	44.163277
3502.848410	666654.000345	44.168282
3503.048884	666599.443848	44.173287
3502.568065	666567.247864	44.178292
3502.730119	666534.646529	44.183297
3502.580690	666514.767176	44.188301
3502.772191	666480.664257	44.193306
3502.820511	666454.466674	44.198311
3502.669491	666414.134423	44.203316
3502.987130	666376.717911	44.208321
3502.888758	666349.047643	44.213325
3503.086443	666314.394370	44.218330
3502.949348	666279.746250	44.223335
3503.069831	666251.341230	44.228340
3503.107860	666209.380602	44.233345
3503.007601	666175.424445	44.238349
3503.085696	666140.041946	44.243354
3503.491026	666094.528211	44.248359
3503.008982	666052.103834	44.253364
3503.358444	666003.705409	44.258369
3503.229264	665973.395090	44.263373
3503.178829	665943.969680	44.268378
3502.935180	665894.720569	44.273383
3503.214428	665867.784892	44.278388
3503.173658	665830.574969	44.283393
3503.222398	665780.877984	44.288397
3503.199572	665757.633649	44.293402
3503.197697	665711.137526	44.298407
3502.887517	665676.465851	44.303412
3502.705772	665633.042232	44.308417
3502.835778	665605.232399	44.313421
3502.800911	665574.755605	44.318426
3503.128915	665540.576953	44.323431
3503.014449	665517.696366	44.328436
3503.102929	665479.316307	44.333441
3502.759354	665442.005100	44.338445
3502.839900	665409.114018	44.343450
3503.357869	665367.020720	44.348455
3502.624215	665334.463111	44.353460
3502.884816	665292.012764	44.358465
3502.825547	665266.827483	44.363469
3502.954618	665227.042767	44.368474
3502.857145	665202.911336	44.373479
3503.000524	665172.803025	44.378484
3502.559286	665131.265889	44.383489
3502.565787	665109.312341	44.388493
3502.654844	665084.102138	44.393498
3502.878495	665058.769904	44.398503
3502.509435	665025.452668	44.403508
3502.939028	664997.392135	44.408513
3503.037582	664956.813041	44.413517
3502.800242	664929.361137	44.418522
3502.874282	664884.445073	44.423527
3502.688980	664860.127678	44.428532
3502.717631	664833.030816	44.433537
3502.926379	664798.270448	44.438541
3502.704519	664758.142463	44.443546
3502.772964	664733.134310	44.448551
3502.861477	664708.422152	44.453556
3502.705923	664665.488772	44.458561
3502.894912	664636.169574	44.463565
3502.940186	664592.703829	44.468570
3502.708219	664568.543069	44.473575
3502.887857	664536.081719	44.478580
3502.806378	664502.415904	44.483585
3503.127072	664475.718968	44.488589
3503.127558	664451.120443	44.493594
3503.025405	664397.499395	44.498599
3502.673972	664366.871342	44.503604
3503.136011	664322.637154	44.508609
3503.044285	664289.471244	44.513613
3502.536976	664268.348886	44.518618
3503.105639	664221.951112	44.523623
3502.915871	664192.643077	44.528628
3503.216878	664158.214471	44.533633
3503.039267	664118.326004	44.538637
3502.573501	664090.110980	44.543642
3503.384607	664055.248667	44.548647
3503.046041	664024.068525	44.553652
3502.843194	663974.403635	44.558657
3503.059723	663939.938270	44.563661
3502.802758	663906.947963	44.568666
3503.128103	663870.917567	44.573671
3502.965704	663849.787350	44.578676
3503.035971	663802.421808	44.583681
3503.247383	663769.503545	44.588685
3502.849360	663730.098879	44.593690
3503.044477	663691.494504	44.598695
3502.995497	663659.866264	44.603700
3503.454963	663618.224051	44.608705
3503.187042	663582.889137	44.613709
3502.554828	663547.863625	44.618714
3502.555581	663504.899301	44.623719
3502.738993	663488.601557	44.628724
3502.808461	663465.635864	44.633729
3502.879348	663426.801396	44.638733
3502.740474	663400.077405	44.643738
3503.195570	663367.666526	44.648743
3502.888902	663337.476923	44.653748
3503.166890	663288.278173	44.658753
3502.880640	663258.833483	44.663757
3502.985540	663226.928954	44.668762
3502.470330	663192.631395	44.673767
3502.624001	663167.505324	44.678772
3502.741273	663128.612108	44.683777
3503.104026	663098.610861	44.688781
3502.902964	663072.045915	44.693786
3502.930370	663029.524204	44.698791
3502.829116	663000.996398	44.703796
3502.703403	662972.622248	44.708801
3503.061363	662931.592638	44.713805
3502.819492	662898.596383	44.718810
3503.137670	662865.258210	44.723815
3502.666968	662833.746652	44.728820
3502.908428	662803.964093	44.733825
3503.039988	662766.614092	44.738829
3502.870089	662733.006559	44.743834
3502.688273	662693.611923	44.748839
3502.567114	662674.668137	44.753844
3502.761667	662635.610484	44.758849
3502.999348	662617.106504	44.763853
3502.762022	662572.979534	44.768858
3503.064357	662542.088218	44.773863
3503.011289	662508.161216	44.778868
3502.848984	662477.745505	44.783873
3502.647490	662450.530141	44.788877
3502.671219	662416.190912	44.793882
3503.009226	662381.550242	44.798887
3502.596344	662355.517288	44.803892
3502.800279	662318.902226	44.808897
3502.808178	662289.605729	44.813901
3502.816248	662254.170555	44.818906
3503.230055	662218.668391	44.823911
3502.657486	662195.506029	44.828916
3502.808621	662148.418480	44.833921
3503.006576	662116.944116	44.838925
3502.666105	662080.817123	44.843930
3502.847196	662046.151201	44.848935
3502.739601	662011.882084	44.853940
3502.695386	661980.546998	44.858945
3502.829129	661945.439341	44.863949
3502.807480	661927.925041	44.868954
3502.802853	661882.658578	44.873959
3502.658733	661861.271440	44.878964
3502.609811	661830.535552	44.883969
3502.703937	661799.276901	44.888973
3502.497093	661776.901725	44.893978
3502.657041	661756.961535	44.898983
3502.787354	661718.559588	44.903988
3502.853288	661691.148285	44.908993
3502.758126	661659.271544	44.913997
3502.674522	661623.599614	44.919002
3502.603033	661589.822153	44.924007
3502.716016	661569.839407	44.929012
3502.750910	661535.894495	44.934017
3502.854544	661505.581633	44.939021
3502.907622	661477.073803	44.944026
3502.952119	661443.276718	44.949031
3502.620540	661407.395296	44.954036
3502.994624	661378.185431	44.959041
3503.270543	661343.551279	44.964045
3502.752317	661300.762488	44.969050
3503.051837	661266.623291	44.974055
3502.580900	661240.696720	44.979060
3502.573696	661204.561445	44.984065
3502.821395	661178.715937	44.989069
3502.658399	661148.695457	44.994074
3502.409262	661113.647877	44.999079
3502.553057	661089.765857	45.004084
3502.483624	661066.917177	45.009089
3502.745983	661029.638742	45.014093
3502.765040	661003.031829	45.019098
3502.739688	660969.244600	45.024103
3502.338088	660946.699941	45.029108
3502.460316	660917.280621	45.034113
3502.791540	660893.566889	45.039117
3502.592336	660873.334666	45.044122
3502.727885	660833.530752	45.049127
3502.754933	660798.736008	45.054132
3502.393406	660773.938188	45.059137
3502.650140	660754.978283	45.064141
3502.391902	660720.330096	45.069146
3502.570591	660704.327932	45.074151
3502.055351	660679.555200	45.079156
3502.433694	660645.850067	45.084161
3502.164495	660622.584020	45.089165
3502.115159	660606.519439	45.094170
3502.219524	660579.997140	45.099175
3502.411719	660554.308863	45.104180
3502.233589	660536.767916	45.109185
3502.118627	660527.053330	45.114189
3502.430214	660503.042385	45.119194
3502.585218	660474.914141	45.124199
3502.138500	660445.936559	45.129204
3501.950304	660443.322074	45.134209
3502.279457	660409.025229	45.139213
3502.191380	660388.623932	45.144218
3502.297263	660364.047541	45.149223
3502.287217	660337.443599	45.154228
3502.088833	660314.664312	45.159233
3502.174736	660298.477102	45.164237
3502.072061	660273.086257	45.169242
3502.472610	660262.238196	45.174247
3502.756454	660230.943226	45.179252
3502.139118	660207.683633	45.184257
3502.714376	660170.550010	45.189261
3502.342490	660161.775914	45.194266
3502.435879	660120.528409	45.199271
3502.631659	660103.124735	45.204276
3502.581566	660076.776268	45.209281
3502.593677	660057.755477	45.214285
3502.382931	660029.536458	45.219290
3502.823616	659992.823681	45.224295
3502.729905	659958.095742	45.229300
3502.385507	659947.519843	45.234305
3502.766339	659902.530048	45.239309
3502.524972	659883.800281	45.244314
3502.387077	659855.269236	45.249319
3502.472760	659834.189190	45.254324
3502.630419	659813.796111	45.259329
3502.563810	659776.217639	45.264333
3502.608960	659746.657717	45.269338
3502.668711	659722.736266	45.274343
3502.558808	659697.844309	45.279348
3502.499166	659664.407630	45.284353
3502.499337	659641.594045	45.289357
3502.634385	659615.613184	45.294362
3502.603718	659586.614396	45.299367
3502.389814	659568.079177	45.304372
3502.437451	659534.424690	45.309377
3502.585041	659501.851883	45.314381
3502.568490	659477.592954	45.319386
3502.448911	659450.705106	45.324391
3502.435196	659426.395662	45.329396
3502.156010	659397.686870	45.334401
3502.510478	659372.717560	45.339405
3502.433051	659352.512019	45.344410
3502.588493	659325.678351	45.349415
3502.457345	659307.827908	45.354420
3502.437791	659283.219535	45.359425
3502.567113	659252.196494	45.364429
3502.619076	659221.785174	45.369434
3502.587947	659197.078645	45.374439
3502.663116	659164.167183	45.379444
3502.759931	659147.776569	45.384449
3502.985882	659104.256377	45.389453
3502.741299	659077.987177	45.394458
3502.739189	659048.832311	45.399463
3502.472529	659017.474386	45.404468
3502.501392	658994.954100	45.409473
3502.843556	658958.253662	45.414477
3502.468764	658932.654537	45.419482
3503.073451	658897.308486	45.424487
3503.000996	658872.508096	45.429492
3502.748629	658856.074682	45.434497
3502.868739	658815.166715	45.439501
3502.763803	658787.975075	45.444506
3503.000981	658751.940185	45.449511
3502.752418	658713.738569	45.454516
3502.661807	658685.745480	45.459521
3502.660453	658646.953688	45.464525
3502.613472	658626.342220	45.469530
3502.756326	658587.226872	45.474535
3503.006411	658560.375504	45.479540
3502.786513	658523.815978	45.484545
3502.898139	658488.250139	45.489549
3502.511757	658462.901320	45.494554
3502.577634	658428.391258	45.499559
3502.709362	658405.153686	45.504564
3502.672823	658383.092106	45.509569
3502.556284	658360.744097	45.514573
3502.476670	658336.991991	45.519578
3502.594637	658298.678423	45.524583
3502.625029	658280.699624	45.529588
3502.421803	658253.173197	45.534593
3502.669949	658210.643916	45.539597
3502.457126	658192.105897	45.544602
3503.024216	658160.158474	45.549607
3502.544649	658126.086721	45.554612
3502.441767	658097.744469	45.559617
3502.843157	658062.428902	45.564621
3502.458105	658041.272764	45.569626
3502.660825	658005.839944	45.574631
3502.784983	657980.355812	45.579636
3502.599714	657952.076643	45.584641
3502.715952	657924.546576	45.589645
3502.539232	657898.013366	45.594650
3502.718242	657867.477031	45.599655
3502.871194	657831.352766	45.604660
3502.659705	657802.628117	45.609665
3502.706063	657771.564113	45.614669
3502.486186	657747.384316	45.619674
3502.231419	657719.565297	45.624679
3502.458085	657683.777853	45.629684
3502.507887	657671.337016	45.634689
3502.718158	657640.794823	45.639693
3502.424382	657619.822452	45.644698
3502.779751	657579.769300	45.649703
3502.555863	657567.872742	45.654708
3502.402546	657542.133605	45.659713
3502.605832	657510.743327	45.664717
3502.562007	657479.144010	45.669722
3502.393877	657456.253185	45.674727
3502.546709	657427.167808	45.679732
3502.298370	657409.532927	45.684737
3502.521884	657365.456143	45.689741
3502.492428	657363.363917	45.694746
3502.412566	657331.170875	45.699751
3502.250799	657307.130210	45.704756
3502.263219	657286.006801	45.709761
3502.681986	657257.676019	45.714765
3501.897858	657224.550092	45.719770
3502.439214	657213.625524	45.724775
3502.114793	657200.546695	45.729780
3502.287889	657175.052403	45.734785
3502.677949	657154.615478	45.739789
3502.178761	657130.679913	45.744794
3502.083415	657095.492649	45.749799
3502.433360	657091.090838	45.754804
3502.164543	657069.863506	45.759809
3502.668365	657037.423516	45.764813
3502.369994	656987.488908	45.769818
3502.231775	656906.867951	45.774823
3502.339318	656777.219614	45.779828
3502.220712	656582.290626	45.784833
3502.136491	656335.916757	45.789837
3501.913767	656031.580632	45.794842
3501.936542	655663.919872	45.799847
3501.614739	655245.810013	45.804852
3501.195097	654779.002008	45.809857
3500.996917	654234.666334	45.814861
3500.758467	653649.447470	45.819866
3500.264607	652997.897020	45.824871
3500.331647	652294.055468	45.829876
3499.746075	651525.421512	45.834881
3499.341491	650696.489682	45.839885
3498.637122	649820.466493	45.844890
3498.267700	648870.998312	45.849895
3497.502099	647867.977060	45.854900
3496.578056	646814.046973	45.859905
3496.193006	645686.131718	45.864909
3495.282177	644522.729798	45.869914
3494.218572	643288.416169	45.874919
3493.404479	641996.451621	45.879924
3492.555537	640649.212462	45.884929
3491.632879	639246.483879	45.889933
3490.743348	637797.181585	45.894938
3489.813279	636280.984093	45.899943
3488.431462	634701.133624	45.904948
3487.623862	633075.201708	45.909953
3486.323260	631388.376023	45.914957
3485.032693	629662.225255	45.919962
3483.724726	627862.233258	45.924967
3482.390181	626029.085110	45.929972
3481.006224	624136.319512	45.934977
3479.686608	622199.670596	45.939981
3477.892081	620206.477104	45.944986
3476.485853	618163.133770	45.949991
3475.216092	616081.236703	45.954996
3473.183754	613955.198622	45.960001
3472.002787	611758.802761	45.965005
3469.920278	609533.932909	45.970010
3468.409177	607263.224093	45.975015
3466.471752	604948.321808	45.980020
3464.624701	602578.526891	45.985025
3463.038032	600177.677087	45.990029
3460.845882	597721.395833	45.995034
3458.715628	595240.328902	46.000039
3456.639850	592705.882864	46.005044
3454.265081	590151.197447	46.010049
3452.406803	587544.016411	46.015053
3450.129407	584915.479209	46.020058
3447.986446	582232.553773	46.025063
3445.785300	579521.693207	46.030068
3443.307037	576767.629405	46.035073
3441.171465	573973.658312	46.040077
3438.531415	571157.511681	46.045082
3435.877743	568307.976116	46.050087
3433.881556	565434.742194	46.055092
3431.068779	562524.648820	46.060097
3428.641480	559570.831275	46.065101
3425.860018	556605.782487	46.070106
3423.283193	553612.176538	46.075111
3420.775710	550578.935656	46.080116
3417.907886	547519.067570	46.085121
3415.160974	544436.415837	46.090125
3412.180986	541333.099298	46.095130
3409.434611	538195.162717	46.100135
3406.573964	535037.684898	46.105140
3403.968701	531850.759168	46.110145
3400.802822	528647.078530	46.115149
3397.713163	525422.749013	46.120154
3394.666280	522175.903086	46.125159
3392.137709	518902.213926	46.130164
3388.633890	515622.128641	46.135169
3385.850499	512298.029146	46.140173
3382.337723	508972.592681	46.145178
3379.094673	505616.190398	46.150183
3376.171674	502259.547712	46.155188
3372.281892	498873.806128	46.160193
3369.518182	495471.006191	46.165197
3366.189016	492070.804581	46.170202
3362.867563	488637.948190	46.175207
3359.746031	485208.383551	46.180212
3356.164339	481751.148443	46.185217
3352.999554	478282.549009	46.190221
3349.221403	474797.644368	46.195226
3346.255728	471297.568755	46.200231
3342.524877	467798.594164	46.205236
3338.821536	464281.042268	46.210241
3335.453339	460752.009399	46.215245
3332.025828	457216.888111	46.220250
3328.167452	453666.976937	46.225255
3324.306218	450122.339650	46.230260
3321.018433	446570.977192	46.235265
3317.459885	443007.507931	46.240269
3313.539575	439435.503606	46.245274
3310.212194	435849.689523	46.250279
3306.805338	432265.203002	46.255284
3302.957114	428668.615014	46.260289
3299.260683	425077.397971	46.265293
3295.338937	421478.681674	46.270298
3291.812088	417871.686817	46.275303
3288.298744	414258.185839	46.280308
3284.490804	410639.813196	46.285313
3280.453594	407021.292256	46.290317
3276.965599	403406.723323	46.295322
3273.088674	399785.527778	46.300327
3269.166434	396154.736248	46.305332
3265.267966	392529.948757	46.310337
3261.571871	388892.825628	46.315341
3257.731615	385263.867729	46.320346
3253.692045	381641.599025	46.325351
3249.801235	378019.772816	46.330356
3245.774972	374388.557089	46.335361
3242.267500	370763.161090	46.340365
3238.255492	367134.739010	46.345370
3234.073791	363522.118441	46.350375
3230.597827	359902.456764	46.355380
3226.171910	356292.291895	46.360385
3222.631405	352669.329282	46.365389
3218.472501	349065.297898	46.370394
3214.571365	345461.673004	46.375399
3210.834714	341848.913726	46.380404
3206.802777	338256.091132	46.385409
3202.808256	334651.684283	46.390413
3198.614959	331054.601040	46.395418
3194.963010	327463.892296	46.400423
3190.853806	323861.204125	46.405428
3186.522069	320285.098962	46.410433
3182.768230	316708.780884	46.415437
3178.734972	313151.903987	46.420442
3174.551635	309576.830843	46.425447
3170.921316	306018.947099	46.430452
3166.700748	302472.088986	46.435457
3162.765796	298929.529374	46.440461
3158.477785	295390.901127	46.445466
3154.560909	291868.955786	46.450471
3150.640091	288349.863274	46.455476
3146.465599	284838.514229	46.460481
3142.647957	281322.442352	46.465485
3138.093290	277831.125513	46.470490
3134.099758	274345.948416	46.475495
3130.306863	270862.804426	46.480500
3126.022216	267396.716918	46.485505
3122.395443	263933.983364	46.490509
3118.067011	260476.595478	46.495514
3114.114438	257035.056939	46.500519
3110.236805	253600.717224	46.505524
3105.888069	250162.852296	46.510529
3102.226992	246739.694327	46.515533
3098.260335	243327.851085	46.520538
3094.120865	239914.983877	46.525543
3090.317017	236513.217220	46.530548
3085.762088	233136.465732	46.535553
3082.164614	229753.438349	46.540557
3077.972094	226375.809346	46.545562
3073.823139	223010.434221	46.550567
3069.952208	219665.889331	46.555572
3065.782255	216319.436976	46.560577
3061.825624	212986.228242	46.565581
3057.953925	209665.197138	46.570586
3053.685277	206352.548085	46.575591
3049.983861	202995.519426	46.580596
3045.574649	199666.266912	46.585601
3041.655363	196373.126091	46.590605
3037.706815	193103.624014	46.595610
3033.424174	189843.663682	46.600615
3029.851023	186587.162323	46.605620
3025.568561	183342.175213	46.610625
3021.746550	180108.528562	46.615629
3017.541855	176875.959589	46.620634
3013.675351	173660.363032	46.625639
3009.501942	170457.435563	46.630644
3005.229911	167258.523370	46.635649
3001.131249	164086.396345	46.640653
2996.817222	160912.870967	46.645658
2993.106563	157761.323995	46.650663
2988.846388	154613.647923	46.655668
2985.111594	151493.197553	46.660673
2981.188765	148364.577594	46.665677
2977.096374	145266.814593	46.670682
2972.776904	142158.307495	46.675687
2968.912167	139073.085792	46.680692
2964.237963	136003.541890	46.685697
2960.805586	132939.795431	46.690701
2956.482262	129892.472099	46.695706
2952.479349	126856.139121	46.700711
2948.344475	123829.832986	46.705716
2944.276028	120829.964767	46.710721
2940.031363	117828.359053	46.715725
2935.983275	114852.512401	46.720730
2931.967604	111883.907391	46.725735
2927.960537	108930.336895	46.730740
2923.262570	105986.762535	46.735745
2919.371205	103064.227682	46.740749
2915.006720	100158.347035	46.745754
2910.801446	97266.693929	46.750759
2906.808788	94389.254428	46.755764
2902.454843	91537.203309	46.760769
2898.296344	88688.810552	46.765773
2893.856488	85866.616642	46.770778
2889.280412	83069.629824	46.775783
2885.153824	80279.223958	46.780788
2880.811875	77527.815733	46.785793
2876.664898	74779.915171	46.790797
2872.516707	72056.879998	46.795802
2867.899004	69356.659692	46.800807
2863.243549	66685.207325	46.805812
2858.715877	64027.266668	46.810817
2853.773622	61405.188022	46.815821
2849.090633	58816.874373	46.820826
2844.218420	56265.109081	46.825831
2838.718250	53739.446137	46.830836
2831.408900	51316.166511	46.835841
2823.249638	48977.117846	46.840845
2814.854829	46712.138453	46.845850
2806.726570	44529.144116	46.850855
2798.597108	42439.466292	46.855860
2790.560618	40462.297508	46.860865
2782.761300	38560.325554	46.865869
2775.849016	36771.109204	46.870874
2768.585131	35069.783899	46.875879
2762.429132	33440.889745	46.880884
2755.877210	31917.129646	46.885889
2749.677254	30452.920458	46.890893
2743.928758	29079.425301	46.895898
2738.204599	27766.802801	46.900903
2732.941995	26510.170153	46.905908
2727.554393	25328.459939	46.910913
2722.645075	24194.344564	46.915917
2717.617143	23110.678581	46.920922
2712.912658	22081.085357	46.925927
2708.818145	21095.972901	46.930932
2703.902552	20151.341532	46.935937
2699.607234	19235.863738	46.940941
2695.325570	18366.750420	46.945946
2691.477137	17512.786027	46.950951
2687.430005	16689.835114	46.955956
2683.196979	15895.557053	46.960961
2679.569102	15119.419583	46.965965
2675.822619	14385.033111	46.970970
2671.676554	13657.617040	46.975975
2667.724166	12945.541432	46.980980
2663.977047	12263.187720	46.985985
2660.021438	11587.933673	46.990989
2656.335566	10943.030072	46.995994
2652.148302	10307.064017	47.000999
2647.530881	9699.518393	47.006004
2643.352168	9118.438802	47.011009
2639.079605	8566.479481	47.016013
2634.544541	8019.496336	47.021018
2630.190498	7500.009934	47.026023
2626.317598	7007.005451	47.031028
2621.624068	6535.031673	47.036033
2617.657125	6078.570708	47.041037
2613.255695	5645.023052	47.046042
2609.296087	5222.196594	47.051047
2605.176289	4833.145069	47.056052
2600.832875	4451.356802	47.061057
2597.090040	4080.234083	47.066061
2593.241693	3726.131671	47.071066
2589.588225	3398.108429	47.076071
2585.715089	3079.634414	47.081076
2581.940538	2761.291529	47.086081
2578.259839	2443.512796	47.091085
2574.809034	2157.671560	47.096090
2571.168661	1866.599631	47.101095
2567.789124	1577.107250	47.106100
2563.899430	1314.225086	47.111105
2560.512311	1047.788656	47.116109
2556.777088	794.914501	47.121114
2552.868083	553.879575	47.126119
2549.042216	320.382658	47.131124
2543.530696	140.189899	47.136129
2531.047071	172.838012	47.141133
2523.049665	167.490088	47.146138
2517.895408	187.028097	47.151143
2515.456130	177.083775	47.156148
2513.948308	175.607951	47.161153
2511.970951	166.633305	47.166157
2510.113514	167.782003	47.171162
2507.195772	180.394018	47.176167
2504.607210	164.939522	47.181172
2501.263088	170.877779	47.186177
2497.772293	172.994071	47.191181
2494.477110	162.350369	47.196186
2491.007426	162.576600	47.201191
2487.767883	163.530530	47.206196
2484.388602	168.076045	47.211201
2481.119278	159.534506	47.216205
2478.006012	156.794493	47.221210
2474.481062	163.653408	47.226215
2471.435002	159.017108	47.231220
2468.265684	157.241681	47.236225
2464.383325	166.737264	47.241229
2461.491111	163.694956	47.246234
2457.741246	167.872045	47.251239
2454.852120	163.058687	47.256244
2451.182361	168.426733	47.261249
2447.438655	156.125639	47.266253
2444.274625	160.073817	47.271258
2440.797995	160.871347	47.276263
2437.676945	155.291333	47.281268
2433.758976	159.647941	47.286273
2430.314345	158.843907	47.291277
2427.051747	158.056005	47.296282
2423.698821	154.773434	47.301287
2420.889420	149.702832	47.306292
2416.726775	160.228060	47.311297
2413.055395	158.960419	47.316301
2410.265994	152.507899	47.321306
2406.495994	164.343194	47.326311
2403.268380	158.241066	47.331316
2400.069512	156.223492	47.336321
2396.934192	158.132770	47.341325
2393.336211	150.416961	47.346330
2389.240622	160.953439	47.351335
2386.216028	154.709866	47.356340
2382.494812	164.154433	47.361345
2378.742528	152.495387	47.366349
2375.739171	150.133164	47.371354
2372.344545	152.603677	47.376359
2369.146902	155.032005	47.381364
2365.628591	161.216172	47.386369
2361.560134	156.983955	47.391373
2358.119010	149.621372	47.396378
2354.946375	161.661001	47.401383
2351.357091	148.703608	47.406388
2348.270646	149.058093	47.411393
2344.295299	152.851951	47.416397
2340.980000	156.659791	47.421402
2337.601742	156.332889	47.426407
2334.183805	149.567990	47.431412
2330.562953	155.886326	47.436417
2327.254107	155.303072	47.441421
2323.831128	148.849234	47.446426
2320.305566	155.153029	47.451431
2316.737403	150.469825	47.456436
2312.782312	154.378768	47.461441
2309.121735	149.523945	47.466445
2306.273964	143.636842	47.471450
2302.452339	156.831911	47.476455
2300.040817	145.974996	47.481460
2296.140869	142.894326	47.486465
2292.563518	147.159676	47.491469
2289.131059	145.015174	47.496474
2285.488939	148.193024	47.501479
2282.121329	145.790553	47.506484
2278.248068	151.902143	47.511489
2274.700690	147.457283	47.516493
2271.426479	151.744432	47.521498
2267.737737	151.195128	47.526503
2264.499840	149.056213	47.531508
2260.920885	148.082268	47.536513
2257.724646	146.874438	47.541517
2254.351947	151.398880	47.546522
2250.756400	154.162544	47.551527
2246.996383	158.363561	47.556532
2243.715880	150.250308	47.561537
2240.442202	153.738752	47.566541
2236.877438	149.521759	47.571546
2232.948308	155.330416	47.576551
2229.422537	147.368380	47.581556
2225.922944	147.436141	47.586561
2222.533331	156.922951	47.591565
2219.401949	142.772930	47.596570
2215.881984	150.518819	47.601575
2212.503607	146.735413	47.606580
2208.840039	146.136412	47.611585
2205.166010	148.789532	47.616589
2202.056321	140.895774	47.621594
2198.100336	141.236252	47.626599
2194.883101	145.138501	47.631604
2191.373121	149.701437	47.636609
2187.798451	150.416663	47.641613
2184.310422	141.423449	47.646618
2180.591717	146.222537	47.651623
2177.591196	146.787515	47.656628
2173.772235	146.796352	47.661633
2170.268874	138.853559	47.666637
2166.950575	141.577027	47.671642
2163.474543	155.613609	47.676647
2159.832694	141.521482	47.681652
2156.643077	144.220157	47.686657
2152.851343	157.750404	47.691661
2149.561000	150.702905	47.696666
2146.067040	151.899565	47.701671
2142.599819	142.290603	47.706676
2138.870556	154.391271	47.711681
2135.492247	152.896067	47.716685
2131.995560	146.689384	47.721690
2128.245368	151.342942	47.726695
2124.699680	148.762980	47.731700
2121.652161	145.935190	47.736705
2117.662730	144.034541	47.741709
2114.373552	134.788912	47.746714
2110.798717	144.050419	47.751719
2107.626394	139.485936	47.756724
2103.936233	141.363682	47.761729
2100.380953	148.272834	47.766733
2096.994007	134.510466	47.771738
2093.406109	137.054719	47.776743
2090.196466	140.309688	47.781748
2086.744170	142.216051	47.786753
2083.032081	131.073797	47.791757
2079.829223	136.814921	47.796762
2076.171079	137.354369	47.801767
2072.929190	136.054350	47.806772
2068.844661	142.665912	47.811777
2065.467788	141.157695	47.816781
2062.045502	135.891542	47.821786
2058.618849	141.461840	47.826791
2055.017752	136.577078	47.831796
2051.591062	138.921277	47.836801
2047.753426	139.796265	47.841805
2044.383072	131.174274	47.846810
2040.765081	148.342462	47.851815
2037.847173	139.126747	47.856820
2034.223166	149.349577	47.861825
2030.486456	141.565811	47.866829
2027.297499	134.038908	47.871834
2023.442772	143.700722	47.876839
2020.067311	136.734086	47.881844
2016.643797	141.952432	47.886849
2012.851648	150.428962	47.891853
2009.463276	146.783916	47.896858
2006.211848	147.025161	47.901863
2002.694363	146.057834	47.906868
1999.074802	138.009850	47.911873
1995.785200	145.034248	47.916877
1991.939015	134.698842	47.921882
1988.468232	138.557251	47.926887
1984.816765	141.039066	47.931892
1981.258569	138.268678	47.936897
1978.089211	141.815245	47.941901
1974.717238	128.026044	47.946906
1971.117088	134.436709	47.951911
1967.719082	135.550553	47.956916
1964.213152	140.692163	47.961921
1960.828304	145.338585	47.966925
1957.422660	135.842749	47.971930
1953.462192	150.837026	47.976935
1950.044276	141.269217	47.981940
1946.313376	144.951375	47.986945
1942.991453	140.416257	47.991949
1939.666837	133.668228	47.996954
1936.014254	136.830492	48.001959
1932.513316	134.668752	48.006964
1929.582496	131.558764	48.011969
1925.487014	129.212248	48.016973
1922.199865	126.474101	48.021978
1918.623136	136.900934	48.026983
1915.406560	133.049783	48.031988
1911.711945	135.817815	48.036993
1908.010673	134.846185	48.041997
1904.865731	127.333617	48.047002
1901.015863	136.653511	48.052007
1897.707662	138.516075	48.057012
1893.911056	130.298905	48.062017
1890.366900	132.495076	48.067021
1887.157326	121.709079	48.072026
1883.277879	139.320739	48.077031
1880.231088	136.361563	48.082036
1876.657380	138.004550	48.087041
1873.194187	135.593696	48.092045
1869.461235	125.828959	48.097050
1865.914137	137.776364	48.102055
1863.063577	133.812692	48.107060
1859.120809	137.098133	48.112065
1855.635894	139.219028	48.117069
1852.315872	124.238107	48.122074
1848.340782	138.071939	48.127079
1845.191612	137.496586	48.132084
1841.594740	130.558379	48.137089
1837.908743	135.307119	48.142093
1834.451995	131.824664	48.147098
1831.128357	138.408994	48.152103
1827.712717	134.236762	48.157108
1824.301927	133.977364	48.162113
1820.575768	137.166469	48.167117
1816.996324	132.634916	48.172122
1813.635913	137.083214	48.177127
1810.035246	130.418186	48.182132
1806.685246	130.550738	48.187137
1803.078544	142.704976	48.192141
1799.691786	124.923041	48.197146
1796.176630	132.342790	48.202151
1792.755049	137.681735	48.207156
1789.145616	134.107319	48.212161
1785.405201	136.607133	48.217165
1782.124153	125.026104	48.222170
1778.485634	135.731813	48.227175
1774.976558	130.433452	48.232180
1771.325897	125.121189	48.237185
1767.875709	134.456254	48.242189
1764.673710	130.448287	48.247194
1761.175169	135.938104	48.252199
1757.796650	133.425138	48.257204
1754.490527	127.387186	48.262209
1750.442623	137.263248	48.267213
1747.008985	133.488927	48.272218
1743.534705	142.942054	48.277223
1740.089199	127.363892	48.282228
1736.478028	133.788183	48.287233
1732.754800	139.488602	48.292237
1729.557877	122.795269	48.297242
1725.952329	127.976191	48.302247
1722.924844	127.473368	48.307252
1719.077764	131.608442	48.312257
1715.537287	133.224942	48.317261
1711.881145	125.780400	48.322266
1708.307405	127.963633	48.327271
1705.080134	135.470466	48.332276
1701.974500	123.203977	48.337281
1698.321013	133.575155	48.342285
1694.652230	122.420182	48.347290
1690.905731	132.806929	48.352295
1687.830896	128.128566	48.357300
1683.730958	127.925509	48.362305
1680.096991	133.704163	48.367309
1677.102785	130.838660	48.372314
1673.441946	130.686201	48.377319
1670.241322	128.848211	48.382324
1666.759496	129.915335	48.387329
1662.817655	135.143975	48.392333
1659.609462	135.736483	48.397338
1655.719801	136.009222	48.402343
1652.362812	125.056743	48.407348
1649.071826	136.129788	48.412353
1645.387242	130.550708	48.417357
1642.069323	123.440086	48.422362
1638.498388	137.291745	48.427367
1635.091346	124.899873	48.432372
1631.972483	120.029121	48.437377
1628.211340	127.315573	48.442381
1624.637241	122.128328	48.447386
1620.989808	126.913279	48.452391
1617.477445	124.320907	48.457396
1613.946719	127.672253	48.462401
1610.421213	125.596125	48.467405
1607.018163	122.450713	48.472410
1603.064613	128.838525	48.477415
1600.340308	126.869584	48.482420
1596.755605	123.007664	48.487425
1593.094403	126.347827	48.492429
1589.752689	134.248189	48.497434
1585.970915	127.548748	48.502439
1582.357383	124.362554	48.507444
1579.011958	126.830409	48.512449
1575.329782	131.577721	48.517453
1571.794638	129.468483	48.522458
1568.354584	119.809348	48.527463
1564.719557	125.927679	48.532468
1561.301518	119.548033	48.537473
1557.827086	128.870067	48.542477
1554.708686	121.005667	48.547482
1551.253787	125.942378	48.552487
1547.569337	127.625024	48.557492
1544.216763	124.695298	48.562497
1540.210082	113.896461	48.567501
1537.054161	123.343869	48.572506
1533.507568	130.353986	48.577511
1529.950624	123.963573	48.582516
1526.011415	116.069866	48.587521
1522.817328	123.164014	48.592525
1519.217805	115.608855	48.597530
1515.748799	127.015292	48.602535
1512.336151	127.991767	48.607540
1509.100056	121.133150	48.612545
1505.269911	123.953092	48.617549
1502.135514	130.487213	48.622554
1498.650314	127.942936	48.627559
1494.842466	121.135206	48.632564
1491.533395	118.662669	48.637569
1487.878860	128.931148	48.642573
1484.555792	122.626446	48.647578
1480.748086	125.322718	48.652583
1477.161873	117.908661	48.657588
1474.135490	123.544619	48.662593
1470.553916	132.415937	48.667597
1467.121179	114.858791	48.672602
1463.339467	126.925335	48.677607
1459.839780	126.140583	48.682612
1456.200548	120.596996	48.687617
1452.625404	127.393827	48.692621
1449.721044	122.576951	48.697626
1446.495490	123.805536	48.702631
1442.330069	114.764870	48.707636
1438.885756	123.217066	48.712641
1435.065191	129.722155	48.717645
1432.066497	120.983195	48.722650
1428.642088	130.236660	48.727655
1425.123250	126.080418	48.732660
1421.674573	122.541106	48.737665
1417.477183	117.596174	48.742669
1414.186195	118.552809	48.747674
1410.464350	127.964573	48.752679
1406.822701	123.879952	48.757684
1403.736419	123.502895	48.762689
1400.445461	132.730968	48.767693
1396.865382	125.827463	48.772698
1393.243471	131.329241	48.777703
1389.364665	126.862910	48.782708
1386.339689	126.141836	48.787713
1382.820026	121.863810	48.792717
1379.546919	120.491294	48.797722
1375.745753	125.846686	48.802727
1372.172138	121.291250	48.807732
1368.766606	129.598159	48.812737
1364.854923	120.920368	48.817741
1362.020508	122.268475	48.822746
1358.378004	123.012703	48.827751
1355.002521	127.389994	48.832756
1351.489161	125.726471	48.837761
1347.683024	132.499399	48.842765
1344.425457	116.641107	48.847770
1340.850839	122.238113	48.852775
1337.543943	121.702795	48.857780
1333.915494	113.258835	48.862785
1330.168321	124.845951	48.867789
1326.727328	119.096838	48.872794
1323.092083	117.574848	48.877799
1319.607457	112.499563	48.882804
1316.420052	122.466763	48.887809
1312.438207	121.789059	48.892813
1309.374467	125.138816	48.897818
1305.603977	122.573572	48.902823
1302.278602	120.010924	48.907828
1299.120413	119.595305	48.912833
1294.929102	129.409180	48.917837
1292.188708	123.883307	48.922842
1288.146281	125.941664	48.927847
1284.642717	119.343325	48.932852
1281.296517	113.410646	48.937857
1277.710626	126.750534	48.942861
1274.305945	123.223404	48.947866
1270.642488	120.154058	48.952871
1266.865247	125.022299	48.957876
1263.777045	113.469427	48.962881
1259.951747	127.279889	48.967885
1256.942885	106.882254	48.972890
1253.955359	119.449128	48.977895
1249.748757	119.806966	48.982900
1246.485913	123.090615	48.987905
1242.502593	126.109551	48.992909
1239.252289	115.745223	48.997914
1235.614905	124.568893	49.002919
1232.094300	127.471283	49.007924
1228.697293	117.894321	49.012929
1225.242322	118.717173	49.017933
1221.916508	112.392614	49.022938
1218.028775	114.688311	49.027943
1214.389062	117.389780	49.032948
1211.342511	117.508312	49.037953
1207.857286	123.950634	49.042957
1204.378333	121.473836	49.047962
1200.717888	118.579089	49.052967
1197.104048	119.553932	49.057972
1193.605890	110.515685	49.062977
1189.761325	121.011540	49.067981
1186.667433	107.860846	49.072986
1183.098821	123.229327	49.077991
1179.610939	113.604089	49.082996
1176.203118	115.240106	49.088001
1172.659898	112.006120	49.093005
1169.132975	111.384756	49.098010
1165.770395	111.004801	49.103015
1161.730857	119.837979	49.108020
1158.767910	118.078279	49.113025
1155.149724	125.471687	49.118029
1151.723423	112.764534	49.123034
1148.470020	105.732647	49.128039
1144.539701	120.253399	49.133044
1141.204475	107.611715	49.138049
1137.410724	120.299914	49.143053
1134.179773	117.701653	49.148058
1130.915947	110.453444	49.153063
1127.116058	118.128517	49.158068
1123.507972	110.785876	49.163073
1120.185288	115.376800	49.168077
1116.471661	110.072351	49.173082
1113.339353	119.968202	49.178087
1109.241530	114.726099	49.183092
1105.992552	111.655258	49.188097
1102.677883	120.442829	49.193101
1099.317163	107.314224	49.198106
1095.254179	107.691084	49.203111
1092.024724	115.163326	49.208116
1088.713862	109.566157	49.213121
1084.848727	114.180099	49.218125
1081.482254	107.462375	49.223130
1078.132465	113.767934	49.228135
1074.719568	114.041659	49.233140
1071.776371	113.904023	49.238145
1067.191327	118.766868	49.243149
1063.684474	116.707231	49.248154
1060.233280	113.500744	49.253159
1057.088375	117.033595	49.258164
1053.904808	110.388855	49.263169
1050.073014	114.283347	49.268173
1046.688126	112.016677	49.273178
1043.035033	123.867078	49.278183
1039.370621	117.760668	49.283188
1036.294243	113.955857	49.288193
1032.255533	112.537726	49.293197
1029.090078	108.473156	49.298202
1025.692855	114.646288	49.303207
1021.753023	120.813247	49.308212
1018.509090	112.355514	49.313217
1014.960591	122.830167	49.318221
1011.564160	111.889896	49.323226
1008.239200	116.254533	49.328231
1004.547866	116.086538	49.333236
1001.082720	110.029503	49.338241
997.203817	117.642556	49.343245
993.790612	115.990974	49.348250
990.420883	103.956418	49.353255
987.008130	115.725270	49.358260
983.727492	108.939163	49.363265
979.902158	113.292241	49.368269
976.423165	111.421063	49.373274
973.077478	102.928893	49.378279
969.200897	111.083271	49.383284
965.997516	107.428969	49.388289
962.205916	116.066788	49.393293
959.082476	114.781523	49.398298
955.613465	116.650815	49.403303
951.876333	124.838589	49.408308
948.688971	118.122922	49.413313
944.461031	116.856542	49.418317
941.122521	109.414817	49.423322
938.149129	111.121049	49.428327
934.675524	105.300893	49.433332
931.194647	109.479034	49.438337
927.251237	114.033429	49.443341
923.716625	113.056549	49.448346
920.266402	109.445869	49.453351
916.857953	110.385385	49.458356
913.555792	107.080763	49.463361
909.705591	112.029231	49.468365
906.450368	111.332157	49.473370
903.093443	110.703411	49.478375
899.213670	109.779098	49.483380
896.076218	101.517379	49.488385
892.477479	105.843902	49.493389
888.788386	110.271806	49.498394
885.268744	109.950994	49.503399
882.027627	116.683906	49.508404
878.710633	113.941212	49.513409
874.745173	109.650121	49.518413
871.313105	108.258688	49.523418
867.959777	100.940842	49.528423
864.120726	103.915120	49.533428
861.276510	102.893364	49.538433
857.342255	108.309059	49.543437
854.031331	105.586498	49.548442
850.466734	105.267426	49.553447
846.701856	113.711665	49.558452
843.153582	104.306685	49.563457
839.745426	107.618002	49.568461
836.176805	97.445797	49.573466
833.005429	96.258342	49.578471
828.892832	111.162301	49.583476
825.829675	108.286691	49.588481
822.433386	98.300499	49.593485
819.137327	101.196641	49.598490
815.582103	105.251790	49.603495
811.604793	106.208719	49.608500
808.435231	99.729004	49.613505
805.046631	106.710532	49.618509
801.311084	105.588793	49.623514
797.753624	105.224973	49.628519
794.173148	106.597578	49.633524
790.869233	104.368037	49.638529
787.054741	109.610847	49.643533
783.916637	103.675923	49.648538
780.159447	105.030805	49.653543
776.604964	108.512600	49.658548
773.499933	96.590155	49.663553
769.961733	107.561734	49.668557
766.106373	100.258347	49.673562
762.986823	102.587983	49.678567
758.903467	99.102696	49.683572
755.614108	97.982372	49.688577
752.055513	107.000154	49.693581
748.674453	107.090470	49.698586
745.340634	101.531319	49.703591
741.889020	99.375979	49.708596
738.529018	95.953388	49.713601
734.594733	103.475952	49.718605
730.892970	101.117306	49.723610
727.744983	98.834393	49.728615
724.137312	110.979415	49.733620
720.829693	94.845624	49.738625
717.408632	101.229915	49.743629
714.118098	95.682970	49.748634
710.377533	103.646126	49.753639
706.332569	101.153652	49.758644
703.008996	95.256187	49.763649
699.275809	104.599289	49.768653
696.137756	95.507441	49.773658
692.824556	97.621504	49.778663
689.070877	105.918175	49.783668
685.834711	92.314686	49.788673
682.256801	104.168868	49.793677
678.719731	97.428005	49.798682
675.208023	97.148674	49.803687
671.876847	98.850729	49.808692
668.475810	97.525366	49.813697
664.947411	100.057492	49.818701
661.444722	104.504660	49.823706
657.767230	104.301315	49.828711
653.853398	100.106679	49.833716
650.868282	90.328097	49.838721
646.894348	106.182118	49.843725
643.578756	94.235419	49.848730
640.041762	97.871700	49.853735
636.569470	105.318105	49.858740
633.147422	101.887905	49.863745
629.387168	98.815788	49.868749
625.651690	97.477120	49.873754
622.943778	106.453505	49.878759
619.092936	107.476311	49.883764
616.149733	91.090713	49.888769
611.867864	95.791355	49.893773
608.600934	101.609521	49.898778
605.219240	97.868376	49.903783
601.430136	102.521637	49.908788
598.160762	98.059593	49.913793
594.539293	107.074669	49.918797
590.752106	95.216112	49.923802
587.658544	84.072596	49.928807
583.925625	109.404104	49.933812
580.743824	90.656237	49.938817
576.925452	97.951360	49.943821
573.797153	106.607197	49.948826
570.579502	102.838935	49.953831
566.420045	108.698254	49.958836
562.927466	100.497933	49.963841
559.486576	99.252857	49.968845
556.020008	104.780660	49.973850
552.972800	100.522640	49.978855
548.964529	101.520447	49.983860
545.557992	103.173498	49.988865
541.640688	96.664791	49.993869
538.390110	107.764171	49.998874
534.940195	100.561255	50.003879
531.484153	103.228330	50.008884
528.085293	98.417961	50.013889
524.641434	101.272862	50.018893
521.194859	100.488945	50.023898
517.930914	93.452413	50.028903
513.752299	104.426146	50.033908
510.721846	94.181962	50.038913
506.683491	102.951929	50.043917
503.533671	95.937567	50.048922
500.165524	99.935754	50.053927
496.523973	105.741004	50.058932
492.949712	99.814944	50.063937
489.620932	108.285758	50.068941
485.999031	101.648692	50.073946
482.541773	96.086901	50.078951
478.802918	104.796080	50.083956
475.780373	94.878983	50.088961
472.098294	103.549367	50.093965
468.174283	105.385203	50.098970
465.060842	101.699235	50.103975
461.354603	102.917686	50.108980
458.386458	107.857306	50.113985
454.817962	106.888192	50.118989
451.053252	104.221707	50.123994
447.538360	99.201500	50.128999
443.857384	105.184603	50.134004
440.482586	96.489322	50.139009
436.768337	103.587358	50.144013
433.201663	96.045101	50.149018
430.137150	104.443208	50.154023
426.295134	104.484160	50.159028
423.028926	92.525146	50.164033
419.426642	99.941713	50.169037
415.868738	101.928745	50.174042
412.596089	88.969724	50.179047
408.823464	99.203632	50.184052
405.312739	103.752374	50.189057
401.660378	108.921304	50.194061
398.215646	98.629543	50.199066
394.969056	99.572469	50.204071
391.190970	93.665831	50.209076
388.028254	88.702044	50.214081
384.447592	90.739044	50.219085
381.015044	99.039040	50.224090
377.707502	100.693595	50.229095
374.074190	100.953430	50.234100
370.303223	102.415725	50.239105
366.902012	105.637245	50.244109
363.600926	93.432254	50.249114
359.850099	99.811787	50.254119
355.885892	102.000502	50.259124
352.705458	100.993687	50.264129
349.205891	107.022419	50.269133
345.755565	101.186287	50.274138
342.213667	100.760077	50.279143
338.445976	99.755556	50.284148
335.131415	99.503662	50.289153
332.578622	100.224051	50.294157
328.706747	96.894016	50.299162
324.959729	96.727525	50.304167
321.305750	100.831172	50.309172
317.782922	96.617917	50.314177
314.292546	97.801551	50.319181
310.719935	94.758850	50.324186
307.407921	95.460081	50.329191
303.650207	96.184967	50.334196
300.166460	94.803732	50.339201
296.894642	106.175550	50.344205
293.190735	101.631165	50.349210
290.187470	94.490300	50.354215
286.329915	100.530777	50.359220
282.966157	91.787238	50.364225
279.515529	100.429519	50.369229
275.829235	101.310934	50.374234
272.214373	101.847031	50.379239
268.529013	108.755516	50.384244
265.212678	99.778978	50.389249
261.335010	101.276592	50.394253
258.151475	94.481923	50.399258
255.212749	96.475318	50.404263
251.172401	101.916584	50.409268
247.855699	90.322671	50.414273
244.520460	101.307585	50.419277
240.823342	98.433358	50.424282
237.095292	93.396725	50.429287
233.788022	107.146819	50.434292
230.575457	100.606998	50.439297
226.621235	98.895620	50.444301
222.925620	101.850644	50.449306
219.656065	91.044410	50.454311
216.027706	101.653202	50.459316
213.168166	96.969109	50.464321
209.209344	98.512172	50.469325
205.470348	92.214633	50.474330
202.146847	92.902651	50.479335
198.446833	93.237417	50.484340
195.135869	95.143687	50.489345
191.792278	97.283874	50.494349
188.280033	92.582353	50.499354
185.092482	87.365317	50.504359
181.164669	96.202700	50.509364
177.688348	98.853869	50.514369
174.358000	102.571350	50.519373
170.617886	91.277500	50.524378
167.082688	85.364610	50.529383
163.580004	100.869238	50.534388
160.032077	92.699957	50.539393
156.931843	93.597715	50.544397
153.163143	90.991956	50.549402
149.986985	85.025360	50.554407
145.919000	84.569593	50.559412
142.837179	86.438556	50.564417
139.303857	92.953343	50.569421
135.403588	81.163904	50.574426
132.283663	94.814163	50.579431
128.398738	95.857056	50.584436
124.877564	89.696987	50.589441
121.681609	93.245436	50.594445
118.429533	99.203564	50.599450
114.913112	87.753151	50.604455
111.018483	91.620544	50.609460
107.792285	84.753540	50.614465
103.993505	88.572705	50.619469
100.309650	94.192274	50.624474
97.432996	80.297534	50.629479
93.751989	88.854556	50.634484
90.464669	86.155929	50.639489
86.803369	84.754544	50.644493
82.987371	89.937794	50.649498
79.471135	89.071840	50.654503
75.664919	93.914654	50.659508
72.505366	89.285669	50.664513
68.937650	90.937164	50.669517
65.867531	86.613256	50.674522
62.320495	81.450716	50.679527
58.377766	89.966644	50.684532
55.030799	90.876914	50.689537
51.575962	83.573030	50.694541
47.786649	86.617320	50.699546
44.661326	81.759704	50.704551
41.080757	90.975811	50.709556
37.711292	86.193159	50.714561
34.178403	90.546349	50.719565
30.670080	92.648225	50.724570
27.224908	95.273833	50.729575
23.359994	101.281019	50.734580
19.824772	91.392754	50.739585
16.639357	93.941019	50.744589
13.013880	91.030075	50.749594
9.634674	86.180783	50.754599
5.978786	87.525867	50.759604
2.452856	93.044376	50.764609