Tue Jun 21 10:40:22 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.527173	78.770003	0.000000
0.821714	73.851496	0.005005
0.632568	71.587512	0.010010
0.771722	73.834099	0.015014
0.873386	80.772997	0.020019
0.255665	62.242472	0.025024
0.517010	60.622779	0.030029
-0.410278	48.525917	0.035034
-0.547817	42.881347	0.040038
-0.615285	42.005788	0.045043
-0.886681	23.377507	0.050048
-1.121647	7.738146	0.055053
-1.641555	8.859936	0.060058
-1.954197	-1.300411	0.065062
-2.176682	-5.795834	0.070067
-2.669913	-3.209907	0.075072
-2.600984	-12.533791	0.080077
-3.394748	1.030622	0.085082
-3.748819	-9.334400	0.090086
-3.994067	-6.191619	0.095091
-4.138451	-0.180328	0.100096
-3.749361	-4.505496	0.105101
-4.240898	-0.641918	0.110106
-5.152816	-6.573424	0.115110
-5.294498	-12.328583	0.120115
-5.673391	-7.456146	0.125120
-5.395172	-6.203677	0.130125
-5.638039	-8.902753	0.135130
-5.346633	-6.850900	0.140134
-6.296375	-3.417604	0.145139
-7.051588	1.312914	0.150144
-6.775331	-8.532324	0.155149
-7.019314	8.045895	0.160154
-6.989006	-2.225903	0.165158
-7.105118	0.912465	0.170163
-7.671921	-8.085130	0.175168
-8.269483	-8.199404	0.180173
-8.672484	0.603173	0.185178
-8.588968	-6.849447	0.190182
-8.650772	-3.834527	0.195187
-8.762614	-3.008232	0.200192
-8.746371	-6.356030	0.205197
-9.772224	3.413026	0.210202
-10.058491	-0.971985	0.215206
-9.844061	-3.461840	0.220211
-9.909152	-2.818322	0.225216
-10.002230	-5.804656	0.230221
-10.831220	0.125040	0.235226
-11.393338	-6.362658	0.240230
-11.595683	-2.672474	0.245235
-11.893126	-4.504901	0.250240
-11.755741	-8.544877	0.255245
-12.175603	-3.914886	0.260250
-11.916346	-9.112868	0.265254
-12.138672	-4.237941	0.270259
-12.728225	-1.758606	0.275264
-13.138739	-5.214122	0.280269
-12.867995	-2.883173	0.285274
-13.277439	-6.041879	0.290278
-13.713606	-0.356216	0.295283
-14.851863	0.108635	0.300288
-14.564285	-7.407181	0.305293
-14.938037	3.772369	0.310298
-14.882344	1.708992	0.315302
-14.775625	-2.542777	0.320307
-14.725958	0.687328	0.325312
-15.177313	-7.692392	0.330317
-15.916815	6.220411	0.335322
-16.010661	-0.071725	0.340326
-16.263652	3.002089	0.345331
-16.343240	8.031575	0.350336
-16.442339	0.427449	0.355341
-17.513350	-0.591338	0.360346
-17.752347	9.414459	0.365350
-17.576333	-2.653720	0.370355
-18.094255	-1.586919	0.375360
-17.981287	-2.843807	0.380365
-18.031097	-0.095101	0.385370
-17.949039	-3.427356	0.390374
-18.925892	1.871090	0.395379
-19.361038	3.792253	0.400384
-19.389230	-0.959319	0.405389
-19.883233	4.791375	0.410394
-19.856272	7.579662	0.415398
-20.017410	1.594670	0.420403
-20.320950	-1.846988	0.425408
-19.884992	-8.191534	0.430413
-20.534340	6.929609	0.435418
-21.097815	-2.885696	0.440422
-21.621512	-4.881539	0.445427
-21.588938	0.270265	0.450432
-21.357750	-3.018014	0.455437
-22.143152	-1.032335	0.460442
-22.516576	-3.750441	0.465446
-22.765842	-5.987090	0.470451
-22.683589	-0.667492	0.475456
-22.859440	-7.691175	0.480461
-22.855650	-7.196013	0.485466
-23.196209	-10.479592	0.490470
-23.640058	1.448012	0.495475
-24.524564	-1.106721	0.500480
-24.169543	-4.388077	0.505485
-24.647149	5.948298	0.510490
-24.959568	5.744379	0.515494
-25.251324	0.126155	0.520499
-25.706302	1.752827	0.525504
-26.025978	-7.269903	0.530509
-26.099629	-1.958626	0.535514
-26.240461	0.615516	0.540518
-26.004827	-7.180199	0.545523
-26.209686	-0.934920	0.550528
-26.160443	-4.098940	0.555533
-27.127612	0.342067	0.560538
-27.674959	0.645523	0.565542
-27.683660	-2.309792	0.570547
-28.082905	5.025387	0.575552
-27.943036	7.431093	0.580557
-27.944888	1.770779	0.585562
-28.418817	-0.480367	0.590566
-28.958743	-5.022675	0.595571
-29.521987	-3.958826	0.600576
-29.315807	-10.285842	0.605581
-29.638009	-2.687357	0.610586
-29.432812	-5.926931	0.615590
-29.671635	-8.627858	0.620595
-31.046717	7.848382	0.625600
-30.996049	1.883371	0.630605
-31.051004	-5.786077	0.635610
-31.001016	2.384412	0.640614
-30.705837	-4.541847	0.645619
-31.337310	4.334878	0.650624
-31.830532	-8.305635	0.655629
-32.386298	-6.092177	0.660634
-32.501760	-15.099387	0.665638
-32.497534	-8.232406	0.670643
-32.674328	2.170380	0.675648
-32.267786	-7.279468	0.680653
-33.321892	-7.549012	0.685658
-34.146267	-3.965385	0.690662
-33.968591	-12.183659	0.695667
-34.537661	-12.494258	0.700672
-34.328317	-9.880626	0.705677
-34.281602	-6.021528	0.710682
-34.516739	-1.830804	0.715686
-34.787351	-3.981038	0.720691
-35.253244	2.717529	0.725696
-35.577738	2.619408	0.730701
-35.601871	-0.607053	0.735706
-35.546033	0.296257	0.740710
-36.047368	-11.539367	0.745715
-36.237516	-3.273070	0.750720
-36.662365	-2.182017	0.755725
-37.237759	2.307974	0.760730
-38.092697	-4.665407	0.765734
-37.754828	-8.850670	0.770739
-38.185055	-5.997723	0.775744
-37.967935	-12.297345	0.780749
-38.365434	-4.055911	0.785754
-38.697064	5.069724	0.790758
-38.148822	-11.978625	0.795763
-39.113465	0.245384	0.800768
-39.670367	-4.731204	0.805773
-40.115640	1.748263	0.810778
-40.229541	-8.018745	0.815782
-40.067716	-10.446805	0.820787
-40.075484	-8.742445	0.825792
-40.501754	-13.473474	0.830797
-40.382614	-4.607001	0.835802
-40.914328	2.439117	0.840806
-41.445690	-10.542777	0.845811
-41.905714	1.992923	0.850816
-41.756285	-7.545374	0.855821
-41.687201	-11.373350	0.860826
-42.359229	-3.313384	0.865830
-43.359012	-8.767778	0.870835
-43.089632	-5.084281	0.875840
-42.703480	-14.360448	0.880845
-43.226586	-4.684715	0.885850
-43.488684	-3.412427	0.890854
-43.490348	-1.685594	0.895859
-44.140812	-2.956948	0.900864
-44.341025	-1.479420	0.905869
-44.543894	-2.051154	0.910874
-44.881542	-8.399997	0.915878
-44.800022	-4.544493	0.920883
-45.568562	-0.455662	0.925888
-45.615771	-7.708241	0.930893
-46.086559	-2.818214	0.935898
-46.433087	-10.091473	0.940902
-46.571172	-1.745393	0.945907
-46.706309	1.174718	0.950912
-46.775947	-13.962545	0.955917
-46.601282	1.219857	0.960922
-47.322800	2.790624	0.965926
-47.357094	-5.810500	0.970931
-48.025071	5.731930	0.975936
-48.513588	-6.610597	0.980941
-48.541943	-0.879595	0.985946
-48.451388	-0.488589	0.990950
-48.373099	-8.358687	0.995955
-49.190311	-8.164851	1.000960
-49.830496	-10.594475	1.005965
-49.948797	-10.166711	1.010970
-49.939985	-1.940862	1.015974
-49.901541	-11.126692	1.020979
-50.183939	-2.732638	1.025984
-50.257658	3.657276	1.030989
-51.189952	8.518755	1.035994
-51.600835	-2.863777	1.040998
-51.291077	-9.881840	1.046003
-52.016564	-4.503067	1.051008
-51.566265	-10.966021	1.056013
-51.662944	-11.337090	1.061018
-52.206004	-9.099291	1.066022
-52.913523	-8.246570	1.071027
-53.409729	-7.321101	1.076032
-53.286483	-5.008944	1.081037
-53.240393	-7.881177	1.086042
-53.275658	-7.020598	1.091046
-53.271305	-10.575993	1.096051
-54.106429	-0.145485	1.101056
-54.370697	-9.622766	1.106061
-54.412289	-2.370698	1.111066
-54.621626	-13.258339	1.116070
-55.149547	-15.087716	1.121075
-56.126725	-2.902283	1.126080
-56.172175	-11.536681	1.131085
-56.305441	-8.243133	1.136090
-56.464629	-7.860693	1.141094
-56.329509	-6.923942	1.146099
-56.784956	-4.140621	1.151104
-56.212993	-4.482515	1.156109
-56.547499	-2.772784	1.161114
-57.461258	0.266014	1.166118
-57.647231	-5.107665	1.171123
-58.062833	-3.244594	1.176128
-58.197321	-8.963251	1.181133
-58.222297	-3.875919	1.186138
-58.538292	-1.443659	1.191142
-58.695437	-5.751775	1.196147
-59.361262	-2.834945	1.201152
-59.613785	-5.166167	1.206157
-59.651373	-9.732658	1.211162
-59.809135	-0.319298	1.216166
-59.488641	-6.368655	1.221171
-60.516093	3.728641	1.226176
-60.748598	1.110338	1.231181
-60.719093	2.909758	1.236186
-61.258672	9.186202	1.241190
-61.087723	4.727251	1.246195
-61.421735	1.867843	1.251200
-62.273209	3.574588	1.256205
-62.338521	-4.044993	1.261210
-62.536762	5.341921	1.266214
-62.802124	-1.817896	1.271219
-62.989574	3.364623	1.276224
-62.630816	0.052256	1.281229
-62.949673	10.029442	1.286234
-63.937661	6.383038	1.291238
-63.967150	1.053694	1.296243
-64.556836	1.771857	1.301248
-64.436581	3.170067	1.306253
-64.416926	1.676046	1.311258
-65.026781	1.636829	1.316262
-65.422676	-1.404531	1.321267
-65.898269	3.817814	1.326272
-66.082139	0.705030	1.331277
-65.972698	3.786903	1.336282
-66.016659	7.600833	1.341286
-65.974156	-2.944510	1.346291
-66.441906	4.138772	1.351296
-66.459133	0.683643	1.356301
-66.981097	10.018007	1.361306
-67.425070	5.367460	1.366310
-67.342931	0.599789	1.371315
-67.909803	7.674625	1.376320
-68.613451	-5.228414	1.381325
-69.024992	-0.210656	1.386330
-68.992642	1.430624	1.391334
-68.567154	-1.062219	1.396339
-69.143705	-1.687308	1.401344
-69.293842	-5.412477	1.406349
-69.481028	0.339106	1.411354
-69.584722	4.540032	1.416358
-70.269875	-7.932328	1.421363
-70.545199	2.257078	1.426368
-70.859565	-2.538067	1.431373
-70.713220	3.743374	1.436378
-71.016740	0.092150	1.441382
-71.035122	-2.251406	1.446387
-72.130434	-4.273342	1.451392
-72.249731	-6.787454	1.456397
-72.363374	-7.002977	1.461402
-72.360588	-11.379806	1.466406
-72.285221	-3.653778	1.471411
-72.487204	-0.403509	1.476416
-72.898987	-7.468624	1.481421
-73.356372	-2.637845	1.486426
-73.787935	-4.655254	1.491430
-73.682138	-12.037953	1.496435
-74.117725	-4.441410	1.501440
-74.909150	-6.701929	1.506445
-75.044207	-13.135032	1.511450
-75.458009	0.764675	1.516454
-75.413276	-9.008078	1.521459
-75.643352	-7.286041	1.526464
-75.367926	-10.285252	1.531469
-75.474112	-6.456876	1.536474
-75.850252	-4.561663	1.541478
-76.543884	-15.332584	1.546483
-77.284380	5.281818	1.551488
-77.377697	-0.161077	1.556493
-77.403283	-5.330041	1.561498
-77.453232	4.046520	1.566502
-77.536034	-4.545779	1.571507
-77.559730	-1.712008	1.576512
-77.631257	-6.616632	1.581517
-78.433972	-4.527833	1.586522
-79.066391	-1.938580	1.591526
-78.676610	-5.970826	1.596531
-79.062642	2.934318	1.601536
-79.272398	-2.157970	1.606541
-79.691664	-3.610279	1.611546
-80.395750	4.996880	1.616550
-80.242621	-4.445533	1.621555
-80.635066	6.194051	1.626560
-80.545935	0.728043	1.631565
-80.593094	-4.346969	1.636570
-81.207505	-8.578563	1.641574
-81.638373	0.205739	1.646579
-82.085894	0.669282	1.651584
-82.293749	3.887965	1.656589
-82.364128	-4.670082	1.661594
-82.481972	-0.107470	1.666598
-82.370664	-8.819136	1.671603
-82.675234	3.851646	1.676608
-82.567112	-12.174636	1.681613
-83.430373	-4.911007	1.686618
-83.882968	1.331493	1.691622
-83.788382	-2.814073	1.696627
-84.347993	1.649629	1.701632
-84.433985	-4.340104	1.706637
-85.053684	2.016305	1.711642
-85.447090	-3.446547	1.716646
-84.998118	-8.032446	1.721651
-85.245674	0.382083	1.726656
-85.450328	-7.954022	1.731661
-85.692191	-7.206241	1.736666
-86.233220	1.386739	1.741670
-86.197735	-1.727247	1.746675
-86.962808	0.587976	1.751680
-86.550691	-5.361510	1.756685
-87.222097	2.344343	1.761690
-88.163470	5.933150	1.766694
-87.797875	-0.469802	1.771699
-87.903353	11.245084	1.776704
-87.917829	-6.280760	1.781709
-88.067808	-4.468784	1.786714
-88.419088	3.579113	1.791718
-89.130219	-13.192380	1.796723
-89.370509	-0.759181	1.801728
-89.667308	-6.235664	1.806733
-89.967044	-1.828421	1.811738
-90.468625	-0.900479	1.816742
-90.004146	-7.274813	1.821747
-90.420859	1.824457	1.826752
-90.258413	-14.079197	1.831757
-91.114209	-8.160248	1.836762
-91.616460	-3.656122	1.841766
-91.483380	-4.784128	1.846771
-91.667180	-1.250934	1.851776
-91.763889	-0.901731	1.856781
-92.021545	-0.494298	1.861786
-92.736158	5.286425	1.866790
-92.789280	-4.806969	1.871795
-93.241068	-2.943823	1.876800
-93.438765	-1.676476	1.881805
-93.244489	-1.267327	1.886810
-93.377489	0.707006	1.891814
-93.128521	-8.898092	1.896819
-94.253317	-2.456056	1.901824
-94.975291	-2.759872	1.906829
-95.047749	-5.602801	1.911834
-95.263165	-2.728003	1.916838
-94.946530	-6.544488	1.921843
-95.144713	0.893550	1.926848
-95.672720	-14.351702	1.931853
-96.030535	-6.923145	1.936858
-96.464099	5.043210	1.941862
-96.163278	-14.116865	1.946867
-96.363261	-4.268108	1.951872
-97.286275	-3.815203	1.956877
-97.827013	-7.110612	1.961882
-98.130704	-6.276025	1.966886
-97.894068	-9.347745	1.971891
-98.253728	-10.299620	1.976896
-98.014784	-8.241257	1.981901
-98.145968	-7.095631	1.986906
-98.383931	-2.323292	1.991910
-98.437899	-3.463929	1.996915
-99.689998	-1.515405	2.006912
-98.882964	-2.500091	2.016909
-98.495988	-4.321139	2.026906
-98.196052	-4.789521	2.036902
-97.243191	-4.684962	2.046899
-97.135109	-3.037236	2.056896
-96.442327	-6.216554	2.066893
-95.467494	0.604855	2.076890
-95.489976	-6.279288	2.086886
-95.387611	0.511756	2.096883
-94.037662	1.108730	2.106880
-94.067235	-5.909586	2.116877
-93.890794	-4.495465	2.126874
-92.755117	-2.682033	2.136870
-92.295485	-3.866833	2.146867
-92.262042	2.414000	2.156864
-91.230213	0.979130	2.166861
-90.863328	-3.966573	2.176858
-90.430827	2.689576	2.186854
-89.542428	-1.211122	2.196851
-89.249131	1.044528	2.206848
-89.356569	3.861302	2.216845
-88.515024	2.172435	2.226842
-87.989268	4.479883	2.236838
-87.660403	-2.360103	2.246835
-86.736272	-8.226769	2.256832
-86.370175	0.513448	2.266829
-86.478238	0.756571	2.276826
-85.143431	-3.753517	2.286822
-85.053276	-0.848743	2.296819
-84.454392	-5.662548	2.306816
-83.668426	-2.772442	2.316813
-83.399774	-8.915051	2.326810
-83.035043	-3.853262	2.336806
-82.197570	-1.883940	2.346803
-81.958925	1.607178	2.356800
-81.724811	0.445501	2.366797
-80.865502	0.374294	2.376794
-80.348393	-2.739177	2.386790
-80.132660	-0.684666	2.396787
-79.090984	-1.568121	2.406784
-78.690284	3.082267	2.416781
-78.656343	-1.625133	2.426778
-77.799973	-0.097382	2.436774
-77.241430	1.216312	2.446771
-77.281965	7.603451	2.456768
-76.413672	1.314107	2.466765
-75.634728	0.821127	2.476762
-75.585402	-0.319035	2.486758
-74.669131	2.624379	2.496755
-74.269674	2.774953	2.506752
-74.177053	7.710900	2.516749
-73.795536	1.128341	2.526746
-72.811651	8.191490	2.536742
-72.280831	6.739027	2.546739
-71.473094	5.845909	2.556736
-71.138221	4.029935	2.566733
-71.133887	4.186671	2.576730
-70.727163	7.418186	2.586726
-69.527258	7.185063	2.596723
-69.827354	10.708700	2.606720
-68.780199	3.538534	2.616717
-68.077594	3.889837	2.626714
-68.191657	2.006544	2.636710
-67.262121	3.148940	2.646707
-66.496061	6.562198	2.656704
-66.404452	4.079154	2.666701
-66.268086	-0.620709	2.676698
-65.298280	3.840391	2.686694
-65.039555	2.862346	2.696691
-64.345734	4.067095	2.706688
-63.476407	14.231763	2.716685
-63.374346	8.713842	2.726682
-63.051321	3.433183	2.736678
-62.469923	-1.968113	2.746675
-61.940385	4.970128	2.756672
-61.271452	3.582719	2.766669
-60.488822	3.370691	2.776666
-60.354462	3.317001	2.786662
-60.344301	2.645676	2.796659
-59.336809	9.899741	2.806656
-58.697016	6.919476	2.816653
-58.378299	-1.100197	2.826650
-57.741929	1.752847	2.836646
-57.106750	6.411827	2.846643
-56.702670	-0.058682	2.856640
-56.864621	5.963076	2.866637
-55.944947	3.582567	2.876634
-55.378626	0.740334	2.886630
-54.581669	11.181950	2.896627
-54.024596	2.679813	2.906624
-54.042739	4.571521	2.916621
-53.624860	6.324235	2.926618
-52.649040	5.304096	2.936614
-52.600542	5.108928	2.946611
-51.920333	6.534464	2.956608
-50.811165	7.335917	2.966605
-50.543137	-0.663506	2.976602
-50.223871	5.867957	2.986598
-50.612331	4.658627	2.996595
-49.360298	5.663052	3.006592
-48.664101	5.924332	3.016589
-47.821144	4.641081	3.026586
-47.618690	-0.962618	3.036582
-47.422782	-0.809749	3.046579
-47.187261	-1.151873	3.056576
-46.081092	-2.479702	3.066573
-46.113040	-6.553991	3.076570
-45.352200	-9.168017	3.086566
-44.549175	-1.127289	3.096563
-44.490801	3.237972	3.106560
-43.890886	-1.641601	3.116557
-43.163704	-4.767926	3.126554
-42.746788	-4.395783	3.136550
-42.505953	-1.257913	3.146547
-41.767381	4.288496	3.156544
-41.294127	6.674591	3.166541
-41.038254	0.152161	3.176538
-40.093061	-1.400338	3.186534
-39.584468	0.575644	3.196531
-39.677275	-1.860855	3.206528
-38.383848	-3.604393	3.216525
-38.282538	-1.882436	3.226522
-37.970841	-4.328622	3.236518
-37.199377	-3.142259	3.246515
-36.733163	-5.112363	3.256512
-36.330524	-4.207139	3.266509
-36.239868	1.178643	3.276506
-35.419576	-5.997413	3.286502
-34.411886	2.141610	3.296499
-33.949771	-0.008014	3.306496
-33.582627	-0.359486	3.316493
-33.482126	1.632903	3.326490
-33.352698	3.003441	3.336486
-32.150922	1.614733	3.346483
-31.857340	5.508528	3.356480
-31.080895	4.630478	3.366477
-30.426111	-1.378493	3.376474
-30.164080	2.316222	3.386470
-30.119157	5.626824	3.396467
-29.360850	2.797059	3.406464
-28.624478	0.241818	3.416461
-28.458242	-0.061564	3.426458
-27.489389	-4.070613	3.436454
-27.244852	1.492607	3.446451
-27.091790	3.867315	3.456448
-26.171965	2.782360	3.466445
-25.515841	-5.548863	3.476442
-25.232488	-3.423944	3.486438
-25.000216	-6.156714	3.496435
-24.077384	-2.820389	3.506432
-23.766289	-5.915544	3.516429
-23.698100	-1.687058	3.526426
-22.918664	2.561363	3.536422
-22.069183	3.749432	3.546419
-21.654016	-1.791096	3.556416
-20.916255	-0.959940	3.566413
-20.676617	0.517221	3.576410
-20.576969	-1.946604	3.586406
-19.791756	2.853114	3.596403
-19.228075	-3.328673	3.606400
-18.776141	1.368168	3.616397
-17.865233	-1.503068	3.626394
-17.835838	-0.586812	3.636390
-17.592866	7.529088	3.646387
-16.508731	1.468380	3.656384
-16.277884	2.670574	3.666381
-15.949563	-3.617265	3.676378
-14.923583	-0.930293	3.686374
-14.398948	6.301198	3.696371
-14.489279	3.612761	3.706368
-13.894167	0.567388	3.716365
-13.032854	-1.059535	3.726362
-12.676770	-2.830806	3.736358
-12.482989	5.727731	3.746355
-11.769951	5.667127	3.756352
-11.385003	-0.622780	3.766349
-10.685392	2.863535	3.776346
-9.848219	0.066356	3.786342
-9.551719	0.397586	3.796339
-9.805687	6.531993	3.806336
-9.041863	-1.958933	3.816333
-8.168071	-0.850761	3.826330
-7.253674	-3.639783	3.836326
-6.930036	-4.728949	3.846323
-6.776080	0.320928	3.856320
-6.320921	-6.699619	3.866317
-5.968737	-7.822951	3.876314
-5.463041	-2.263658	3.886310
-4.812314	-5.178545	3.896307
-4.145587	0.477772	3.906304
-3.757952	-1.375585	3.916301
-3.302915	7.325818	3.926298
-2.987523	16.981574	3.936294
-2.623705	26.891515	3.946291
-2.026899	37.188680	3.956288
-1.748028	50.326450	3.966285
-1.178022	66.342283	3.976282
-0.632129	91.685675	3.986278
-0.214843	107.340558	3.996275
0.000000	120.138655	4.001280
0.174138	129.163244	4.006285
0.540208	141.827083	4.011290
0.764562	149.257582	4.016294
0.671357	137.502645	4.021299
0.567760	146.929230	4.026304
0.731865	152.932711	4.031309
1.037466	168.339879	4.036314
1.398126	175.777814	4.041318
1.450082	166.276269	4.046323
1.035775	167.237119	4.051328
0.939415	155.467299	4.056333
1.157054	167.638522	4.061338
1.155151	159.495676	4.066342
1.313329	163.289986	4.071347
0.967397	163.598172	4.076352
1.232315	166.156063	4.081357
1.180918	163.628702	4.086362
1.252924	167.867277	4.091366
1.123286	165.916463	4.096371
1.073376	160.495720	4.101376
1.388204	162.244557	4.106381
1.470658	168.557175	4.111386
0.902944	157.060574	4.116390
1.326446	155.921170	4.121395
1.228856	158.163165	4.126400
1.485922	170.382129	4.131405
1.487500	163.358190	4.136410
1.190575	160.707108	4.141414
1.476798	159.759158	4.146419
1.279774	153.126275	4.151424
1.175792	157.380966	4.156429
1.589020	168.292178	4.161434
1.157295	176.781308	4.166438
1.419360	173.113337	4.171443
1.212250	176.647273	4.176448
1.509655	177.299442	4.181453
1.321885	170.072617	4.186458
1.405563	176.129683	4.191462
1.594535	176.107358	4.196467
1.612665	183.329498	4.201472
1.720759	174.771783	4.206477
1.503980	169.935749	4.211482
1.421407	158.695660	4.216486
1.254845	159.938127	4.221491
1.805718	171.703704	4.226496
1.703481	177.470097	4.231501
1.524081	159.799085	4.236506
1.221743	167.267477	4.241510
1.853228	162.715444	4.246515
1.538322	182.191824	4.251520
1.548204	180.811293	4.256525
1.429102	175.363325	4.261530
1.287882	182.329267	4.266534
1.705012	180.614302	4.271539
1.532793	182.755586	4.276544
1.550990	177.726518	4.281549
1.693281	172.664667	4.286554
1.520735	182.013298	4.291558
1.816390	175.407551	4.296563
1.428953	178.816243	4.301568
1.561628	174.895006	4.306573
1.610116	175.123867	4.311578
1.619613	166.972814	4.316582
1.770791	174.021561	4.321587
1.421467	175.951028	4.326592
1.718589	172.876954	4.331597
1.558986	174.444663	4.336602
1.515420	182.111553	4.341606
1.851291	189.383101	4.346611
1.587134	203.260579	4.351616
2.285947	199.645783	4.356621
1.800505	193.610422	4.361626
1.876679	191.213485	4.366630
1.848716	188.027874	4.371635
2.052441	199.861615	4.376640
2.303364	189.099875	4.381645
1.635898	174.959888	4.386650
1.510227	186.819158	4.391654
2.163244	192.485551	4.396659
2.255123	205.938804	4.401664
1.990668	182.861225	4.406669
1.765653	177.395867	4.411674
1.910552	201.312553	4.416678
2.254496	201.468413	4.421683
1.941323	203.611729	4.426688
2.043656	198.666995	4.431693
1.968336	204.890510	4.436698
1.974430	208.609769	4.441702
2.355253	204.042005	4.446707
1.932323	205.917359	4.451712
1.927085	209.220932	4.456717
2.309107	203.156372	4.461722
2.198292	209.130612	4.466726
2.469164	202.671434	4.471731
1.682874	196.565318	4.476736
1.985135	202.011161	4.481741
2.155594	216.931432	4.486746
2.150449	212.421660	4.491750
2.312803	200.300133	4.496755
2.115046	213.319658	4.501760
2.343259	209.790288	4.506765
2.300908	209.861326	4.511770
2.090251	220.685853	4.516774
2.433508	212.932591	4.521779
2.264374	224.145706	4.526784
2.247186	217.741328	4.531789
2.216825	222.663274	4.536794
1.931091	217.121720	4.541798
2.135080	207.775536	4.546803
2.010147	213.399475	4.551808
2.129992	212.933737	4.556813
2.526150	208.470981	4.561818
1.933939	214.902641	4.566822
2.202586	205.099969	4.571827
2.024977	209.332333	4.576832
2.170686	221.469729	4.581837
2.368972	240.587297	4.586842
2.077310	236.992061	4.591846
2.718710	235.327372	4.596851
2.578735	246.478052	4.601856
2.789436	243.267905	4.606861
2.885400	240.301920	4.611866
1.940811	232.342966	4.616870
2.345324	217.776977	4.621875
2.264660	235.934712	4.626880
2.673806	238.008542	4.631885
2.568727	239.448038	4.636890
2.522309	246.320362	4.641894
3.070084	236.570905	4.646899
2.500987	242.826475	4.651904
2.308005	243.495127	4.656909
2.458258	242.674673	4.661914
2.524715	243.812254	4.666918
2.696287	244.579591	4.671923
2.624650	243.623803	4.676928
2.636164	243.287302	4.681933
2.658520	246.343983	4.686938
2.274968	245.461554	4.691942
2.589628	244.590391	4.696947
2.575136	249.767637	4.701952
2.574445	244.583411	4.706957
2.784309	248.076533	4.711962
2.458014	247.081021	4.716966
2.655932	244.376396	4.721971
2.785188	253.630297	4.726976
2.823759	251.621030	4.731981
2.853864	246.453411	4.736986
3.021611	243.425809	4.741990
2.969625	244.346595	4.746995
2.684987	244.496039	4.752000
2.481802	240.801296	4.757005
2.725554	243.782242	4.762010
2.603760	270.227666	4.767014
3.055561	271.615006	4.772019
3.134600	275.750028	4.777024
2.769547	258.985230	4.782029
2.764865	271.039428	4.787034
2.789434	285.130047	4.792038
2.929146	273.425830	4.797043
2.992689	286.012603	4.802048
3.037426	287.449790	4.807053
3.147082	273.328040	4.812058
2.888806	283.088957	4.817062
3.243333	287.354782	4.822067
3.077936	282.354306	4.827072
3.255920	281.718109	4.832077
2.959471	264.274945	4.837082
2.680654	268.710568	4.842086
2.961977	279.027615	4.847091
3.019599	287.798083	4.852096
2.902786	285.595104	4.857101
3.001789	282.179863	4.862106
2.782960	278.848828	4.867110
3.132317	277.840097	4.872115
2.953538	281.925461	4.877120
2.955684	281.715029	4.882125
2.939848	278.377020	4.887130
2.948833	284.109446	4.892134
2.829434	274.955501	4.897139
3.045476	286.352141	4.902144
3.340556	294.369719	4.907149
3.272195	311.149670	4.912154
3.141172	307.457170	4.917158
3.393254	303.573355	4.922163
3.712603	302.315223	4.927168
3.434081	301.827833	4.932173
3.352580	287.043690	4.937178
3.260591	287.831191	4.942182
3.491110	277.293984	4.947187
3.349723	276.197203	4.952192
3.337686	285.647190	4.957197
3.551040	283.853673	4.962202
3.269167	281.409650	4.967206
3.615672	284.084687	4.972211
3.145065	288.814533	4.977216
3.502820	284.034877	4.982221
3.371302	280.773844	4.987226
3.410727	289.300654	4.992230
3.306966	279.470014	4.997235
3.179426	281.690741	5.002240
3.507901	294.738831	5.007245
3.305772	307.346922	5.012250
3.351946	305.327114	5.017254
3.593613	299.320491	5.022259
3.612002	307.748969	5.027264
3.652423	310.610466	5.032269
3.780476	306.021777	5.037274
3.794207	310.957762	5.042278
3.804150	294.137142	5.047283
3.269666	280.875683	5.052288
3.321180	285.791788	5.057293
3.353699	289.436438	5.062298
3.294316	306.041240	5.067302
3.292007	300.431804	5.072307
3.329702	310.940180	5.077312
3.567916	311.444090	5.082317
3.346915	302.450616	5.087322
3.202967	312.268988	5.092326
3.414971	305.487200	5.097331
3.725118	331.598347	5.102336
3.772486	333.205208	5.107341
4.014084	336.256386	5.112346
3.718324	338.546419	5.117350
3.762974	327.647649	5.122355
3.816119	321.460887	5.127360
3.666779	326.018550	5.132365
3.848504	339.858427	5.137370
3.519596	335.785266	5.142374
3.763176	343.185442	5.147379
3.719324	348.406261	5.152384
3.791317	343.714559	5.157389
3.890991	336.726394	5.162394
3.662405	348.817335	5.167398
3.980554	340.105751	5.172403
3.957252	344.883497	5.177408
3.805392	351.980336	5.182413
3.818264	339.036282	5.187418
3.528943	347.555995	5.192422
3.833305	346.946031	5.197427
4.157523	344.066748	5.202432
3.827689	347.468898	5.207437
4.172620	346.456751	5.212442
3.954705	341.418973	5.217446
4.286220	342.509907	5.222451
4.148736	348.286345	5.227456
4.070765	351.172979	5.232461
3.915920	340.093717	5.237466
3.785023	343.563170	5.242470
3.813592	340.723374	5.247475
3.857159	347.450599	5.252480
3.900570	342.585040	5.257485
3.951047	351.949727	5.262490
3.697703	356.473116	5.267494
4.621110	356.585513	5.272499
4.335557	360.034206	5.277504
4.118267	354.688473	5.282509
4.020584	344.281348	5.287514
4.121889	347.609340	5.292518
4.501470	353.243914	5.297523
4.111714	355.680349	5.302528
4.223874	354.710497	5.307533
4.225636	345.491454	5.312538
3.900476	367.069044	5.317542
4.345270	365.013017	5.322547
4.336903	372.737517	5.327552
4.201205	373.250264	5.332557
4.557871	370.123667	5.337562
4.279452	373.314642	5.342566
4.412251	375.283092	5.347571
4.231452	383.705128	5.352576
4.388627	378.154307	5.357581
4.474273	380.272650	5.362586
4.340751	375.249501	5.367590
4.587208	372.537606	5.372595
4.577208	369.309515	5.377600
4.244870	360.839235	5.382605
4.215278	358.203050	5.387610
4.119787	366.214301	5.392614
4.335684	369.202253	5.397619
4.421386	377.947993	5.402624
4.337374	380.075880	5.407629
4.179882	378.762319	5.412634
4.325281	381.141712	5.417638
4.730384	379.758075	5.422643
4.474697	375.041888	5.427648
4.688260	376.770420	5.432653
4.645672	369.206087	5.437658
4.518901	372.817539	5.442662
4.469628	370.587576	5.447667
4.700333	376.396987	5.452672
4.365397	369.625030	5.457677
4.339949	371.259938	5.462682
4.205250	377.612153	5.467686
4.409007	377.253088	5.472691
4.294170	382.286165	5.477696
4.502275	398.038472	5.482701
4.794045	403.720956	5.487706
5.054403	408.721906	5.492710
5.059736	401.445235	5.497715
4.787280	390.163999	5.502720
4.553775	384.768843	5.507725
4.835021	376.982748	5.512730
4.448827	382.653565	5.517734
4.978671	388.890805	5.522739
4.591008	383.999329	5.527744
4.518098	395.522242	5.532749
4.728990	408.971159	5.537754
4.907522	409.425951	5.542758
5.058266	405.627172	5.547763
4.949511	417.110254	5.552768
5.030221	409.762093	5.557773
4.734641	387.797814	5.562778
4.924567	401.043582	5.567782
4.696261	403.115840	5.572787
4.861949	412.161531	5.577792
4.944090	415.753987	5.582797
5.250189	413.794331	5.587802
4.884146	402.998644	5.592806
4.755372	407.087205	5.597811
4.786730	407.057236	5.602816
4.797862	417.848330	5.607821
4.793547	417.196138	5.612826
4.659391	422.406282	5.617830
5.107593	411.671513	5.622835
4.801527	411.990468	5.627840
4.845197	413.126902	5.632845
5.100358	407.778298	5.637850
4.599424	425.203866	5.642854
4.782325	415.522415	5.647859
4.891668	413.387149	5.652864
4.694121	421.288045	5.657869
5.133643	422.106729	5.662874
5.102966	444.451855	5.667878
5.015095	437.720654	5.672883
5.017897	440.672668	5.677888
5.101106	442.646379	5.682893
5.197630	436.594670	5.687898
5.085821	440.234839	5.692902
4.978017	435.889217	5.697907
5.213421	444.811096	5.702912
4.978240	435.559010	5.707917
5.146755	446.397078	5.712922
5.195864	448.244811	5.717926
5.297992	443.932900	5.722931
5.497466	451.024887	5.727936
5.124714	447.835735	5.732941
5.378063	438.200425	5.737946
5.307506	448.076390	5.742950
5.408204	441.775143	5.747955
5.267827	436.907033	5.752960
5.069820	445.824511	5.757965
5.280181	434.182673	5.762970
5.174783	445.053074	5.767974
5.519710	443.092116	5.772979
5.375972	442.356645	5.777984
4.987018	444.533855	5.782989
5.463162	453.169988	5.787994
5.416365	470.525731	5.792998
5.654440	462.612355	5.798003
5.342751	455.144442	5.803008
5.471803	462.790779	5.808013
5.479947	464.043807	5.813018
5.445892	480.317215	5.818022
5.706563	473.976045	5.823027
5.729929	473.264999	5.828032
5.542823	463.427125	5.833037
5.755919	449.239343	5.838042
5.345190	443.166053	5.843046
5.595697	440.713964	5.848051
5.492661	448.006811	5.853056
5.356490	456.268558	5.858061
5.543758	465.228416	5.863066
5.681195	474.559240	5.868070
5.308247	476.781757	5.873075
5.740956	476.416352	5.878080
5.727126	476.433727	5.883085
5.888101	474.399031	5.888090
5.920748	476.250283	5.893094
5.555155	477.240776	5.898099
5.800797	477.683668	5.903104
5.923806	477.862699	5.908109
6.231075	466.779837	5.913114
5.723835	452.512221	5.918118
5.549626	445.512330	5.923123
5.804744	453.339072	5.928128
5.878570	460.897067	5.933133
5.926452	459.808990	5.938138
5.569623	453.593765	5.943142
5.879237	456.860249	5.948147
5.910366	475.080267	5.953152
5.812159	465.464872	5.958157
5.811680	466.674138	5.963162
5.799835	472.635050	5.968166
5.757020	467.653683	5.973171
6.042736	472.920809	5.978176
6.016248	471.974304	5.983181
6.181173	475.144968	5.988186
6.082809	468.004038	5.993190
5.676514	445.300031	5.998195
6.009868	454.479997	6.003200
5.592042	461.395765	6.008205
5.771745	467.432308	6.013210
5.701959	471.343379	6.018214
5.820021	471.024947	6.023219
5.810419	471.029585	6.028224
5.659920	475.103410	6.033229
5.847576	480.280411	6.038234
5.779465	476.218294	6.043238
5.905869	476.369135	6.048243
6.002670	475.654414	6.053248
5.783569	475.607309	6.058253
6.162839	480.759092	6.063258
5.674503	479.091026	6.068262
5.614427	476.602940	6.073267
6.004006	483.078744	6.078272
6.032117	489.567047	6.083277
6.175937	478.036246	6.088282
5.883302	481.021798	6.093286
5.812051	475.003580	6.098291
5.897726	477.397023	6.103296
6.081994	482.591951	6.108301
6.408173	474.829547	6.113306
5.919984	474.856011	6.118310
5.934405	472.032545	6.123315
6.221679	474.301038	6.128320
6.069871	478.119130	6.133325
6.230605	478.688172	6.138330
6.224153	484.790280	6.143334
6.013742	469.338397	6.148339
6.287394	476.580522	6.153344
6.165378	477.461216	6.158349
6.266336	471.405799	6.163354
6.131798	477.512340	6.168358
6.158500	471.747468	6.173363
6.078356	474.407545	6.178368
5.706707	462.193676	6.183373
5.879816	461.914871	6.188378
5.901648	474.079886	6.193382
6.037737	481.295656	6.198387
6.266211	478.658552	6.203392
5.768900	484.194670	6.208397
6.100868	476.931956	6.213402
5.838454	478.567832	6.218406
6.031087	471.727017	6.223411
6.192026	478.060312	6.228416
5.718100	466.708187	6.233421
5.794914	463.026029	6.238426
5.785676	467.275377	6.243430
6.047700	470.393847	6.248435
5.933452	466.858178	6.253440
6.104245	477.763381	6.258445
6.233927	471.668081	6.263450
5.957911	483.362238	6.268454
6.067518	476.991616	6.273459
6.078996	463.281815	6.278464
6.006101	447.605501	6.283469
5.937653	441.496252	6.288474
5.803923	455.970226	6.293478
5.897143	451.729252	6.298483
5.903045	465.969552	6.303488
5.820598	471.799873	6.308493
6.036104	472.504889	6.313498
5.861608	482.884332	6.318502
5.785135	478.065026	6.323507
6.271168	480.031830	6.328512
5.896652	486.547139	6.333517
5.974158	479.259467	6.338522
5.748739	481.111618	6.343526
5.813317	480.941759	6.348531
5.811123	477.395820	6.353536
5.889702	478.073979	6.358541
5.805174	471.390755	6.363546
5.869470	474.846267	6.368550
5.613197	470.695526	6.373555
6.038755	474.771048	6.378560
5.380629	476.190848	6.383565
5.730385	469.469257	6.388570
5.505406	477.050298	6.393574
5.908841	492.905534	6.398579
5.839149	510.422590	6.403584
6.096345	504.229988	6.408589
6.230853	498.815687	6.413594
5.942725	488.898422	6.418598
6.023675	483.744209	6.423603
6.054146	468.112524	6.428608
5.831062	485.291059	6.433613
6.081007	475.378238	6.438618
5.917531	489.202791	6.443622
6.138642	481.735636	6.448627
6.193194	475.976610	6.453632
5.941669	482.535292	6.458637
6.061931	475.046556	6.463642
5.663518	481.643178	6.468646
5.974425	473.998154	6.473651
6.133393	467.971416	6.478656
5.909365	470.273664	6.483661
5.961539	463.960907	6.488666
5.793227	479.996256	6.493670
5.968191	469.235456	6.498675
5.870139	474.410629	6.503680
5.939093	472.406564	6.508685
6.286965	469.181550	6.513690
6.300189	468.172030	6.518694
6.131200	478.520366	6.523699
6.146007	469.356712	6.528704
5.885601	470.507785	6.533709
5.898681	472.274264	6.538714
5.901331	474.178239	6.543718
5.965060	476.892638	6.548723
6.055328	477.444537	6.553728
5.688628	482.348259	6.558733
5.830641	474.194637	6.563738
5.583835	482.875516	6.568742
5.647322	479.883290	6.573747
6.101807	494.801591	6.578752
5.981451	506.594510	6.583757
6.260519	502.112974	6.588762
5.925277	492.922811	6.593766
5.891451	488.707996	6.598771
6.306744	473.489749	6.603776
6.112540	476.962808	6.608781
6.042135	473.178728	6.613786
5.909240	478.075702	6.618790
6.103892	468.176186	6.623795
6.136225	472.422006	6.628800
5.872660	489.870303	6.633805
5.824646	471.343417	6.638810
5.745031	484.073448	6.643814
5.792968	485.458618	6.648819
6.002014	477.409140	6.653824
5.782632	484.501829	6.658829
5.920900	473.389720	6.663834
5.947302	480.867762	6.668838
5.856638	486.360223	6.673843
6.376739	491.380349	6.678848
5.923668	489.352611	6.683853
6.156053	480.150355	6.688858
5.929112	481.751545	6.693862
5.527222	480.188751	6.698867
6.199327	480.296391	6.703872
5.909045	493.464282	6.708877
5.964459	484.159704	6.713882
6.089971	482.784666	6.718886
6.067616	478.134201	6.723891
6.163361	482.215993	6.728896
6.060388	480.779529	6.733901
5.883935	477.179762	6.738906
5.848289	477.641212	6.743910
6.128252	480.755135	6.748915
6.285358	477.228995	6.753920
6.281709	474.608426	6.758925
6.192601	471.668702	6.763930
5.820829	480.101103	6.768934
6.119451	478.282393	6.773939
5.943349	481.184118	6.778944
6.016296	481.123383	6.783949
5.935593	473.440197	6.788954
6.289134	474.734502	6.793958
6.050630	475.630539	6.798963
6.248674	480.095397	6.803968
6.148596	486.102105	6.808973
6.172638	488.203628	6.813978
6.174019	476.044604	6.818982
6.020565	473.405625	6.823987
6.179651	450.893929	6.828992
5.902743	458.503689	6.833997
6.039632	445.006983	6.839002
5.956686	447.435645	6.844006
6.103431	443.303818	6.849011
6.252510	445.544475	6.854016
5.943898	442.684521	6.859021
6.006141	441.258196	6.864026
5.653836	441.935282	6.869030
5.856300	446.735270	6.874035
5.826735	442.459573	6.879040
5.687157	446.611504	6.884045
5.922251	458.240541	6.889050
5.955913	478.378084	6.894054
5.933069	470.950937	6.899059
6.229363	478.415268	6.904064
6.013517	475.994419	6.909069
6.213497	460.899260	6.914074
5.963755	452.925768	6.919078
5.812267	449.866530	6.924083
5.836670	440.551523	6.929088
5.884565	461.821584	6.934093
6.446845	466.238555	6.939098
5.955963	454.040096	6.944102
5.840487	448.529861	6.949107
5.622496	444.884093	6.954112
5.858750	458.912583	6.959117
6.282971	474.925387	6.964122
5.668799	468.254686	6.969126
6.145220	476.791130	6.974131
6.139211	462.400444	6.979136
5.808750	454.279881	6.984141
5.680920	443.829332	6.989146
6.213265	471.220172	6.994150
5.957686	470.493749	6.999155
6.042175	466.371633	7.004160
5.902327	453.348775	7.009165
5.927879	456.998960	7.014170
5.836504	458.453572	7.019174
6.103324	464.854579	7.024179
6.271652	462.549496	7.029184
5.723776	453.262746	7.034189
5.867076	447.314980	7.039194
6.052571	464.717304	7.044198
5.767516	463.890776	7.049203
6.082682	466.100578	7.054208
5.761654	473.420063	7.059213
6.036891	473.462981	7.064218
5.846690	472.150486	7.069222
6.049192	470.498264	7.074227
6.192820	468.850662	7.079232
5.950256	474.300979	7.084237
6.315118	464.834856	7.089242
6.183460	457.945132	7.094246
6.033797	446.045583	7.099251
6.029224	434.914925	7.104256
5.638604	445.369206	7.109261
5.985713	439.462288	7.114266
6.029577	434.870926	7.119270
5.891441	436.517988	7.124275
5.903596	442.562730	7.129280
5.479882	444.973228	7.134285
6.163621	458.784742	7.139290
6.047127	471.440750	7.144294
5.820022	466.257041	7.149299
6.265734	463.776174	7.154304
5.899542	465.991848	7.159309
6.279087	435.878070	7.164314
6.270522	435.910559	7.169318
5.809326	441.718535	7.174323
5.891677	436.999040	7.179328
5.877823	434.175133	7.184333
5.937984	428.868877	7.189338
6.112510	433.797614	7.194342
5.990255	437.918257	7.199347
6.088016	434.470036	7.204352
5.694206	440.805193	7.209357
5.838699	426.017633	7.214362
5.843049	428.222066	7.219366
6.063224	442.635252	7.224371
5.948701	431.523790	7.229376
6.142247	441.842654	7.234381
6.007152	428.013296	7.239386
6.155524	438.679062	7.244390
5.865556	440.820145	7.249395
5.976736	437.821608	7.254400
5.845214	451.507435	7.259405
5.832971	443.684854	7.264410
5.943371	449.220573	7.269414
5.703095	448.965428	7.274419
6.070426	459.097852	7.279424
5.971003	466.990613	7.284429
6.251385	461.158082	7.289434
5.901028	448.333091	7.294438
6.044337	442.372893	7.299443
6.229656	439.899432	7.304448
6.151479	451.089953	7.309453
6.218141	454.477381	7.314458
6.209838	447.717804	7.319462
5.930166	442.892296	7.324467
6.027062	442.033305	7.329472
5.953195	445.413612	7.334477
5.827146	441.536138	7.339482
5.999803	444.818985	7.344486
5.862930	440.077973	7.349491
6.248366	444.518301	7.354496
5.911451	445.217507	7.359501
5.796552	447.145088	7.364506
5.859319	445.562976	7.369510
5.888461	439.299036	7.374515
5.804748	446.087243	7.379520
5.521321	453.026534	7.384525
5.848482	438.977744	7.389530
6.090780	453.121855	7.394534
5.961069	453.512842	7.399539
6.023554	449.481204	7.404544
6.006897	450.584413	7.409549
6.373998	442.203299	7.414554
6.106626	443.038006	7.419558
6.350976	449.596257	7.424563
6.129106	448.309137	7.429568
6.080157	439.512256	7.434573
6.010757	441.240686	7.439578
6.379099	441.210760	7.444582
6.240019	443.328239	7.449587
6.489942	440.164838	7.454592
5.968773	438.368417	7.459597
6.212819	414.693600	7.464602
6.119302	419.073913	7.469606
5.666695	424.656086	7.474611
6.267349	412.491413	7.479616
5.916523	419.241157	7.484621
6.091759	417.018608	7.489626
6.206827	414.522447	7.494630
5.848095	412.790696	7.499635
5.837047	409.871211	7.504640
5.920601	415.158572	7.509645
5.887585	415.791862	7.514650
5.842951	412.925299	7.519654
5.670724	417.630442	7.524659
5.936078	429.769501	7.529664
5.883350	446.521355	7.534669
6.004958	445.944414	7.539674
6.002414	444.527633	7.544678
5.940446	455.776056	7.549683
5.977466	443.969129	7.554688
5.815432	445.059707	7.559693
5.866399	445.370255	7.564698
5.915972	447.474452	7.569702
5.752123	447.796102	7.574707
5.761231	442.792134	7.579712
6.075670	444.183491	7.584717
5.869466	444.738700	7.589722
6.270573	444.937985	7.594726
6.114751	443.648216	7.599731
5.841419	445.841208	7.604736
6.011928	445.347143	7.609741
5.915672	445.563667	7.614746
6.265256	449.975795	7.619750
5.915242	449.740203	7.624755
5.940766	437.767051	7.629760
5.883093	451.778690	7.634765
6.109667	451.380522	7.639770
6.033076	447.059724	7.644774
5.878426	448.150658	7.649779
5.986735	443.426666	7.654784
6.106085	455.544141	7.659789
6.178635	447.132273	7.664794
5.843702	423.407288	7.669798
5.960316	438.071465	7.674803
6.162110	441.009866	7.679808
5.854236	433.834775	7.684813
5.804510	425.255893	7.689818
6.210937	440.733860	7.694822
5.820143	442.180627	7.699827
5.898033	438.146836	7.704832
5.869617	441.080930	7.709837
6.279901	443.042907	7.714842
5.965668	430.475790	7.719846
5.870636	425.960318	7.724851
5.963521	429.259924	7.729856
5.625440	436.840730	7.734861
6.045159	442.089997	7.739866
5.989184	437.545557	7.744870
6.071854	443.533431	7.749875
6.104531	444.060726	7.754880
6.065394	448.852375	7.759885
5.830975	427.574914	7.764890
6.095828	429.603202	7.769894
5.891283	424.127261	7.774899
6.278784	420.644679	7.779904
5.719823	415.683087	7.784909
5.765581	412.377080	7.789914
6.417573	430.171189	7.794918
6.219224	424.258696	7.799923
6.336646	413.080421	7.804928
5.994151	413.921843	7.809933
5.861728	411.388718	7.814938
6.080128	409.307224	7.819942
6.157742	409.848191	7.824947
5.920607	419.541755	7.829952
6.012498	413.796302	7.834957
5.912847	411.165198	7.839962
6.132750	409.364268	7.844966
6.010011	415.816936	7.849971
5.979490	408.194147	7.854976
5.980123	419.226945	7.859981
6.000707	415.058986	7.864986
6.098278	417.972214	7.869990
5.871359	412.506495	7.874995
5.929343	410.818812	7.880000
5.594049	422.169306	7.885005
5.583179	415.144353	7.890010
5.981913	411.265038	7.895014
5.744524	417.188289	7.900019
5.827450	416.712674	7.905024
5.795097	420.817242	7.910029
5.826709	422.959339	7.915034
6.239313	433.553718	7.920038
5.989093	434.938331	7.925043
6.207829	418.600818	7.930048
5.771883	431.230560	7.935053
5.860178	421.662060	7.940058
5.886147	415.728803	7.945062
5.900811	425.645897	7.950067
5.700374	433.128721	7.955072
6.097120	446.648919	7.960077
6.123633	441.809018	7.965082
6.135875	452.519043	7.970086
5.649654	437.736260	7.975091
6.289222	433.111177	7.980096
5.636249	428.002147	7.985101
5.861408	444.134120	7.990106
6.079894	436.806348	7.995110
6.102493	447.169904	8.000115
5.818572	446.143102	8.005133
5.884891	450.106519	8.010150
5.909421	435.430018	8.015168
5.950634	449.369090	8.020186
5.835809	450.671956	8.025203
6.106289	438.365766	8.030221
5.991277	446.330172	8.035238
5.909348	447.856313	8.040256
6.248940	445.638910	8.045274
5.811618	442.877769	8.050291
6.546650	441.354669	8.055309
6.242613	445.204033	8.060326
6.070069	430.954630	8.065344
5.944208	420.597212	8.070362
5.640279	419.500670	8.075379
6.183998	429.447557	8.080397
5.947151	437.048108	8.085414
5.949460	447.430110	8.090432
5.887583	442.173120	8.095450
6.065828	448.118837	8.100467
5.964293	440.127281	8.105485
5.908880	446.441980	8.110502
5.920333	454.767703	8.115520
5.983859	444.786555	8.120538
5.699146	447.420999	8.125555
5.872591	435.763313	8.130573
5.901286	444.753449	8.135590
6.016884	445.803409	8.140608
5.841298	443.498889	8.145626
6.051167	436.925736	8.150643
5.950464	439.790712	8.155661
6.190228	455.211364	8.160678
6.080476	451.058282	8.165696
6.157843	452.633236	8.170714
6.310411	457.940146	8.175731
5.732004	455.919833	8.180749
6.287535	463.596647	8.185766
6.020865	473.970062	8.190784
6.212172	477.345901	8.195802
6.253727	481.837404	8.200819
6.585052	472.376615	8.205837
6.066379	462.760939	8.210854
6.430721	455.573265	8.215872
6.271637	451.224430	8.220890
6.302307	448.930239	8.225907
6.135251	449.327254	8.230925
5.972684	441.965836	8.235942
5.842181	449.482646	8.240960
6.270238	453.543040	8.245978
6.226328	470.810550	8.250995
6.338322	473.495833	8.256013
6.074121	463.546700	8.261030
6.375515	480.619255	8.266048
6.294608	461.463270	8.271066
6.209467	464.028451	8.276083
6.330152	458.965617	8.281101
6.370813	458.116121	8.286118
5.983986	450.597361	8.291136
6.342340	470.659070	8.296154
6.293488	480.425988	8.301171
6.397325	471.871705	8.306189
6.327147	467.073529	8.311206
6.146034	473.461806	8.316224
6.404696	470.772206	8.321242
6.196679	480.611739	8.326259
6.514853	465.245685	8.331277
6.281743	457.298544	8.336294
6.109013	459.276107	8.341312
6.332895	459.854037	8.346330
6.669674	474.018576	8.351347
6.518649	473.724208	8.356365
6.266605	457.152879	8.361382
6.223766	456.535107	8.366400
6.225544	443.484491	8.371418
6.230279	454.335745	8.376435
6.426272	462.410851	8.381453
6.364159	461.975391	8.386470
6.443592	460.738203	8.391488
6.315488	450.270318	8.396506
6.132066	461.750919	8.401523
6.137177	474.584854	8.406541
6.399503	474.952889	8.411558
6.416152	483.378942	8.416576
6.653659	472.562330	8.421594
6.263916	477.433499	8.426611
6.446553	479.913201	8.431629
6.719556	469.208421	8.436646
6.588101	474.658820	8.441664
6.278338	458.482058	8.446682
6.170017	467.150040	8.451699
6.404976	472.949377	8.456717
6.292786	477.593692	8.461734
6.401406	478.373176	8.466752
6.548086	479.208164	8.471770
6.475517	473.886798	8.476787
6.566839	472.494895	8.481805
6.765896	480.392744	8.486822
6.199941	485.333841	8.491840
6.719277	480.247502	8.496858
6.632486	476.065809	8.501875
6.408962	480.700413	8.506893
6.451231	478.371032	8.511910
6.446270	474.256098	8.516928
6.542469	475.359860	8.521946
6.435602	480.549514	8.526963
6.766514	466.291112	8.531981
6.556255	476.658534	8.536998
6.620063	482.194505	8.542016
6.620041	471.233186	8.547034
6.429098	482.947709	8.552051
6.386064	482.624828	8.557069
6.468821	478.584534	8.562087
6.132385	486.558465	8.567104
6.490167	474.958013	8.572122
6.361974	483.759403	8.577139
6.278232	481.972898	8.582157
6.362562	482.564095	8.587175
6.213711	485.991540	8.592192
6.431091	484.303191	8.597210
6.398360	483.996320	8.602227
6.594437	480.781884	8.607245
6.500156	472.960160	8.612263
6.244296	489.597877	8.617280
6.719378	497.986800	8.622298
6.854147	500.605131	8.627315
6.547534	511.226113	8.632333
6.791082	505.607129	8.637351
6.446441	507.834411	8.642368
6.674152	513.772749	8.647386
6.532783	521.489214	8.652403
6.654872	510.791091	8.657421
6.900064	512.885466	8.662439
6.725995	522.312542	8.667456
6.660565	518.612306	8.672474
7.068147	510.965115	8.677491
6.692578	505.202216	8.682509
6.780697	487.616324	8.687527
6.412314	494.883593	8.692544
6.660492	496.279686	8.697562
6.660226	506.736164	8.702579
6.876113	516.239596	8.707597
6.837746	512.033734	8.712615
6.648952	511.563939	8.717632
6.467560	496.050479	8.722650
6.631983	512.733772	8.727667
6.538648	514.959398	8.732685
6.520895	507.265328	8.737703
6.679639	511.506545	8.742720
6.758966	519.040410	8.747738
6.857290	519.475956	8.752755
6.509707	523.610090	8.757773
7.011071	517.373646	8.762791
6.890430	514.412424	8.767808
6.736158	514.891177	8.772826
7.012076	510.930494	8.777843
6.813463	515.131683	8.782861
6.695200	513.669963	8.787879
6.596604	515.575813	8.792896
6.543405	523.957946	8.797914
6.603294	516.296680	8.802931
6.696510	523.835531	8.807949
7.161836	518.946299	8.812967
6.627609	518.225854	8.817984
6.696647	510.735112	8.823002
6.667075	514.889412	8.828019
6.745761	516.060246	8.833037
6.943519	510.937391	8.838055
6.721648	514.023219	8.843072
7.109786	504.584889	8.848090
6.695855	506.561262	8.853107
6.861477	520.470742	8.858125
6.893015	508.889252	8.863143
6.458410	516.040143	8.868160
6.634941	530.960157	8.873178
7.053384	547.994507	8.878195
7.249818	550.618580	8.883213
7.215701	538.060606	8.888231
6.893704	527.343890	8.893248
6.973397	515.509753	8.898266
6.957130	513.536099	8.903283
6.828051	522.722277	8.908301
7.162191	516.968217	8.913319
6.957123	511.178261	8.918336
6.943173	511.115703	8.923354
6.881184	518.145644	8.928371
6.909319	529.896753	8.933389
7.078882	534.966246	8.938407
6.968034	537.576835	8.943424
6.856565	533.155726	8.948442
6.944421	544.988092	8.953459
7.013335	551.717256	8.958477
6.828023	554.261641	8.963495
7.169504	553.330831	8.968512
7.358033	554.219913	8.973530
7.128530	545.587923	8.978547
7.151899	543.832686	8.983565
7.139694	528.051232	8.988583
6.957211	526.946578	8.993600
6.907395	530.203116	8.998618
6.993178	533.696040	9.003635
7.003683	549.516734	9.008653
7.097690	548.841063	9.013671
7.000313	556.870712	9.018688
7.120726	556.685320	9.023706
7.232939	550.747146	9.028723
7.064620	547.634769	9.033741
7.384403	550.561228	9.038759
7.474517	546.216766	9.043776
7.096129	533.879573	9.048794
7.196448	522.045362	9.053811
7.014382	528.599950	9.058829
7.404311	517.087247	9.063847
7.112143	522.402870	9.068864
6.826559	520.296068	9.073882
7.013137	516.166924	9.078899
7.195391	536.449598	9.083917
7.566717	531.119070	9.088935
7.135283	537.289001	9.093952
7.011876	515.877150	9.098970
7.053833	518.165996	9.103987
7.133827	532.662856	9.109005
7.143409	551.476805	9.114023
7.400883	546.762920	9.119040
7.245444	539.123326	9.124058
7.079262	537.874839	9.129075
7.085780	554.316431	9.134093
7.469126	542.892588	9.139111
7.397947	547.582688	9.144128
6.852081	543.769104	9.149146
7.585182	545.816937	9.154163
7.257878	553.981896	9.159181
7.010346	549.070357	9.164199
7.365213	554.007799	9.169216
7.572787	552.510030	9.174234
7.599387	531.826612	9.179251
7.211060	524.026392	9.184269
7.131346	521.558159	9.189287
7.317718	536.556662	9.194304
7.303971	543.203454	9.199322
7.591295	533.124366	9.204339
7.247537	525.719886	9.209357
7.152342	522.470807	9.214375
7.322477	519.977932	9.219392
7.353545	537.809438	9.224410
7.276733	539.554805	9.229427
7.345358	556.607332	9.234445
7.200478	548.914216	9.239463
7.639240	547.921434	9.244480
7.544419	542.511411	9.249498
7.274727	539.284729	9.254515
7.240201	550.944860	9.259533
7.274572	545.593949	9.264551
7.579168	548.250500	9.269568
7.306708	558.785156	9.274586
7.523053	548.780406	9.279603
7.348112	549.641690	9.284621
7.320956	546.627189	9.289639
7.456660	551.337555	9.294656
7.408911	555.606876	9.299674
7.535761	545.987395	9.304691
7.434124	549.311176	9.309709
7.384732	553.519356	9.314727
7.486531	547.733686	9.319744
7.593617	549.563947	9.324762
7.507976	553.524800	9.329779
7.147131	550.324627	9.334797
7.386841	546.376230	9.339815
7.205641	544.284224	9.344832
7.422541	548.427638	9.349850
7.351196	551.775535	9.354867
7.253629	542.872503	9.359885
7.311786	545.490537	9.364903
7.355390	547.835017	9.369920
7.114093	557.711800	9.374938
7.292458	554.228843	9.379955
7.379313	568.216563	9.384973
7.389349	569.760556	9.389991
7.670510	569.976666	9.395008
7.437904	582.311311	9.400026
7.555630	573.121642	9.405043
7.612407	585.166259	9.410061
7.526567	569.655601	9.415079
7.826455	566.053116	9.420096
7.773463	570.613645	9.425114
7.650373	573.275870	9.430131
7.734425	581.623890	9.435149
7.484695	579.721168	9.440167
7.605087	574.784518	9.445184
7.422345	571.520991	9.450202
7.571852	575.088997	9.455219
7.309213	583.499743	9.460237
7.617941	581.172084	9.465255
7.845004	577.251953	9.470272
7.562134	578.364758	9.475290
7.976574	578.506832	9.480307
7.368583	584.629056	9.485325
7.896518	582.783371	9.490343
8.009945	575.644082	9.495360
7.570337	585.906258	9.500378
7.685578	573.784909	9.505395
7.684321	579.046275	9.510413
7.831645	578.587350	9.515431
7.804907	579.723090	9.520448
7.879740	581.311468	9.525466
7.983028	588.897104	9.530483
7.617347	584.092908	9.535501
7.639348	570.698110	9.540519
8.034853	581.033985	9.545536
7.549957	582.102494	9.550554
7.746989	583.820233	9.555571
7.929416	577.691891	9.560589
7.610442	581.526834	9.565607
7.792249	578.570433	9.570624
7.628994	589.470269	9.575642
7.653556	575.381977	9.580659
7.934979	587.638788	9.585677
7.666757	587.605739	9.590695
7.887520	583.664210	9.595712
7.844485	589.401955	9.600730
7.872132	593.601129	9.605747
7.843351	588.902352	9.610765
7.377393	595.081960	9.615783
7.961927	578.275123	9.620800
7.709313	582.018177	9.625818
7.893374	575.645486	9.630835
7.974038	576.691202	9.635853
8.001731	576.993771	9.640871
8.203180	577.761628	9.645888
8.157014	586.967182	9.650906
8.197228	574.676576	9.655923
7.785916	573.317508	9.660941
7.662893	580.341639	9.665959
8.027619	572.894219	9.670976
7.798501	584.408658	9.675994
8.012483	576.072282	9.681011
8.013892	585.265233	9.686029
8.057118	586.589179	9.691047
8.017576	574.916071	9.696064
7.928684	580.612591	9.701082
7.588230	574.579694	9.706099
7.624828	574.783944	9.711117
7.909258	577.064337	9.716135
7.928963	578.626807	9.721152
7.935217	583.988105	9.726170
8.178133	599.099935	9.731187
8.085377	588.010198	9.736205
7.982167	585.105324	9.741223
7.979998	586.008074	9.746240
7.948345	592.997004	9.751258
8.003262	606.582790	9.756275
8.126768	607.452133	9.761293
7.724199	608.471973	9.766311
8.354283	602.697219	9.771328
8.192093	605.923566	9.776346
7.902624	613.844708	9.781363
8.330653	611.576812	9.786381
8.055949	615.303258	9.791399
8.293500	612.714565	9.796416
8.187669	610.911034	9.801434
8.335022	600.203548	9.806451
8.165075	581.697748	9.811469
7.876308	579.626503	9.816487
8.080393	585.967967	9.821504
8.211684	599.278322	9.826522
8.068205	603.174361	9.831539
7.945354	606.110747	9.836557
7.990167	607.262789	9.841575
7.935645	605.848768	9.846592
7.795880	612.090107	9.851610
7.983565	604.054509	9.856627
8.003453	608.529757	9.861645
7.901025	608.586174	9.866663
8.526164	605.200669	9.871680
7.905911	609.170543	9.876698
8.240250	619.063846	9.881715
8.152152	601.235567	9.886733
8.010349	618.537561	9.891751
8.060275	620.233211	9.896768
8.146433	636.551866	9.901786
8.087279	635.778728	9.906803
8.489956	636.525863	9.911821
8.165872	638.214950	9.916839
8.350568	640.130395	9.921856
8.648791	637.457639	9.926874
8.321774	639.445618	9.931891
8.399667	638.948192	9.936909
8.739530	645.576627	9.941927
8.358935	619.997244	9.946944
8.136522	619.437350	9.951962
8.292536	625.265171	9.956979
8.402580	628.992864	9.961997
8.221868	634.769762	9.967015
8.645100	632.118036	9.972032
8.484949	629.065310	9.977050
8.227959	620.302996	9.982067
8.209180	619.584586	9.987085
8.299471	639.208650	9.992103
8.678788	638.356997	9.997120
8.666375	640.110607	10.002138
8.325634	628.770586	10.007155
8.598594	617.177382	10.012173
8.425596	607.440598	10.017191
8.282212	614.381705	10.022208
8.282297	616.970984	10.027226
8.212587	643.033742	10.032243
8.587622	641.972969	10.037261
8.613926	648.845443	10.042279
8.492174	640.550063	10.047296
8.780137	643.536924	10.052314
8.675057	637.405974	10.057331
8.515576	618.030932	10.062349
8.478122	614.035901	10.067367
8.413494	611.670465	10.072384
8.274241	617.455451	10.077402
8.345160	632.308608	10.082419
8.694850	632.018914	10.087437
8.167309	632.323670	10.092455
8.531572	631.000524	10.097472
8.465788	639.315713	10.102490
8.511944	637.156717	10.107507
8.854584	635.750543	10.112525
8.403248	647.196714	10.117543
8.488362	638.309240	10.122560
8.557984	635.994004	10.127578
8.559477	640.278225	10.132595
8.562504	633.945528	10.137613
8.302594	643.001483	10.142631
8.541883	635.546657	10.147648
8.466811	651.236949	10.152666
8.282533	651.256924	10.157683
8.441104	646.514113	10.162701
8.621757	652.641389	10.167719
8.534217	666.494504	10.172736
8.313651	667.599950	10.177754
8.703381	678.078177	10.182771
8.828072	674.601917	10.187789
9.005596	683.238628	10.192807
8.819718	683.766318	10.197824
8.929715	674.810533	10.202842
8.516081	670.906913	10.207859
8.774050	664.170591	10.212877
8.668068	672.161372	10.217895
8.676161	677.925917	10.222912
8.714691	682.537067	10.227930
8.655140	673.436141	10.232947
8.959624	673.396437	10.237965
8.750757	683.244309	10.242983
8.820928	675.952500	10.248000
8.903296	672.821025	10.253018
8.664341	681.060194	10.258035
9.111020	682.746840	10.263053
8.948412	682.140034	10.268071
9.039997	674.610442	10.273088
8.656030	663.388177	10.278106
8.685464	678.592716	10.283123
9.019124	678.036006	10.288141
9.059132	688.063127	10.293159
8.783603	672.629445	10.298176
8.865194	673.545888	10.303194
8.983498	680.384244	10.308211
8.951226	681.932498	10.313229
8.832600	683.888336	10.318247
9.197920	677.457440	10.323264
9.081582	661.596251	10.328282
8.521187	662.248159	10.333299
8.983179	663.374426	10.338317
8.857024	675.143518	10.343335
8.600992	684.063430	10.348352
8.970253	683.461063	10.353370
8.903494	683.047822	10.358387
9.273977	674.854759	10.363405
9.105647	685.469495	10.368423
8.936093	689.965902	10.373440
9.009538	690.787637	10.378458
8.897634	682.239044	10.383475
9.259443	677.622008	10.388493
9.361484	679.442885	10.393511
9.030861	680.833863	10.398528
8.978542	661.093405	10.403546
9.072469	667.237016	10.408563
8.801718	672.308409	10.413581
9.034969	679.743049	10.418599
9.324927	686.087656	10.423616
9.277355	673.185758	10.428634
9.037343	665.486686	10.433651
9.097976	667.224266	10.438669
8.909618	669.915621	10.443687
8.725516	685.292527	10.448704
9.540945	677.418672	10.453722
8.795448	680.761311	10.458739
8.999797	677.454919	10.463757
8.986891	680.275087	10.468775
8.873604	683.709481	10.473792
8.807237	678.237419	10.478810
9.016443	683.198631	10.483827
9.116545	677.434845	10.488845
8.947536	685.250648	10.493863
8.839876	688.130994	10.498880
9.040659	672.689298	10.503898
8.961272	685.669085	10.508915
9.433465	696.215160	10.513933
9.366440	705.134885	10.518951
9.262693	700.492187	10.523968
9.244688	681.379842	10.528986
9.011753	689.743996	10.534003
9.494302	690.977878	10.539021
9.200048	701.363886	10.544039
9.294454	707.419250	10.549056
9.390078	705.250478	10.554074
9.186079	701.982569	10.559091
9.293971	700.042068	10.564109
9.127551	696.919897	10.569127
9.477400	711.699384	10.574144
9.661754	714.133369	10.579162
9.042699	697.786131	10.584179
9.198605	698.676884	10.589197
9.479230	708.638191	10.594215
9.270530	712.173032	10.599232
9.559367	697.893434	10.604250
9.641363	715.098243	10.609267
9.413548	703.268234	10.614285
9.416028	695.532140	10.619303
9.520376	699.599356	10.624320
9.792884	690.289111	10.629338
9.438390	689.258202	10.634355
9.644738	687.069916	10.639373
9.426897	681.175325	10.644391
9.029337	679.065785	10.649408
9.490165	674.304015	10.654426
9.364287	692.031381	10.659443
9.155806	684.392034	10.664461
9.568946	694.802227	10.669479
9.521646	704.768231	10.674496
9.716631	704.808860	10.679514
9.262580	710.797183	10.684531
9.672552	707.191395	10.689549
9.591108	715.953288	10.694567
9.036452	710.139263	10.699584
9.587959	720.422235	10.704602
9.520909	719.492928	10.709619
9.294264	711.311332	10.714637
9.571637	721.416090	10.719655
9.355281	711.995852	10.724672
9.611737	711.062185	10.729690
9.306560	713.120961	10.734707
9.264028	719.052557	10.739725
9.535947	705.851284	10.744743
9.454798	710.977508	10.749760
9.733098	710.749237	10.754778
9.375267	700.743807	10.759795
9.371728	710.737605	10.764813
9.724106	700.638582	10.769831
9.540158	719.608201	10.774848
9.188731	709.467853	10.779866
9.758171	728.614284	10.784883
9.884140	733.727082	10.789901
10.024384	732.518186	10.794919
9.503611	726.706811	10.799936
9.586263	727.291604	10.804954
9.893261	746.087443	10.809971
9.962286	750.737262	10.814989
9.922243	727.384648	10.820007
9.606825	729.973046	10.825024
9.783776	704.080738	10.830042
9.675555	722.161099	10.835059
10.112213	721.175544	10.840077
9.764261	718.523169	10.845095
9.552484	721.299116	10.850112
9.780153	719.972993	10.855130
10.097394	732.497398	10.860147
9.953663	724.655194	10.865165
9.913786	712.212199	10.870183
9.820107	715.594537	10.875200
9.444538	706.313652	10.880218
9.956403	724.679500	10.885235
9.844018	723.875410	10.890253
9.883994	722.151259	10.895271
9.694652	733.667094	10.900288
9.765535	735.502192	10.905306
9.568869	742.169911	10.910323
9.892073	739.600082	10.915341
10.069694	736.611473	10.920359
9.474964	743.677769	10.925376
9.975166	748.461687	10.930394
9.972300	736.388508	10.935411
9.646852	744.286935	10.940429
10.046172	742.152508	10.945447
9.875109	751.484742	10.950464
9.967370	745.484448	10.955482
9.967273	748.986328	10.960499
9.639277	745.438173	10.965517
10.075276	739.073496	10.970535
9.937352	752.728743	10.975552
9.869897	743.163756	10.980570
9.903540	746.889957	10.985587
9.546452	748.194778	10.990605
10.091383	758.557207	10.995623
10.210805	774.864594	11.000640
10.181824	769.193013	11.005658
10.357622	771.837468	11.010675
10.130415	762.272547	11.015693
10.141984	743.316243	11.020711
9.848518	747.403288	11.025728
10.106340	752.373399	11.030746
10.402706	759.215767	11.035763
10.207711	762.713312	11.040781
10.322693	742.376573	11.045799
9.768949	741.874296	11.050816
9.964067	751.919472	11.055834
10.031682	754.878280	11.060851
10.313190	764.460757	11.065869
10.409764	774.247871	11.070887
10.290201	776.027113	11.075904
10.422853	760.171832	11.080922
10.256199	752.618828	11.085939
9.907107	750.418579	11.090957
10.452967	749.488164	11.095975
10.497879	751.765729	11.100992
10.163650	746.816714	11.106010
10.638455	741.292414	11.111027
10.390084	738.281438	11.116045
10.121394	738.313816	11.121063
10.050586	737.976436	11.126080
10.321671	743.578959	11.131098
10.291655	738.519731	11.136115
10.171314	745.304727	11.141133
10.394506	748.848760	11.146151
10.223447	761.683170	11.151168
10.313512	764.431187	11.156186
10.414154	768.054964	11.161203
10.699994	768.842320	11.166221
10.291520	753.288060	11.171239
10.132008	758.831978	11.176256
10.486225	766.359220	11.181274
10.590405	773.550726	11.186291
10.302172	778.955739	11.191309
10.686143	775.205825	11.196327
10.500856	762.399095	11.201344
10.332382	742.613991	11.206362
10.502638	749.828007	11.211379
10.424287	752.628318	11.216397
10.671243	755.884576	11.221415
10.425495	749.218244	11.226432
10.344185	740.237411	11.231450
10.593986	760.867835	11.236467
10.429429	767.039330	11.241485
10.542789	759.367122	11.246503
10.537953	771.325635	11.251520
10.364449	776.065227	11.256538
10.445691	772.408355	11.261555
10.394270	772.673244	11.266573
10.574674	770.890008	11.271591
10.551710	771.727712	11.276608
10.299609	775.006776	11.281626
10.570765	776.037889	11.286643
10.220300	772.090714	11.291661
10.315513	775.010705	11.296679
10.410457	777.381952	11.301696
10.483136	765.652127	11.306714
10.424770	770.380131	11.311731
10.166491	777.918258	11.316749
10.697202	792.288365	11.321767
10.793117	810.729099	11.326784
10.806735	802.061628	11.331802
11.082071	801.225611	11.336819
10.484592	782.155953	11.341837
10.720835	791.758934	11.346855
10.755179	805.583329	11.351872
10.511304	803.732953	11.356890
11.006423	808.889367	11.361907
10.736527	816.488095	11.366925
10.842821	809.316220	11.371943
10.940623	806.080986	11.376960
10.790903	801.571060	11.381978
10.883353	786.355055	11.386995
10.512083	800.534786	11.392013
10.535540	798.964929	11.397031
11.072663	810.318792	11.402048
11.146075	799.073835	11.407066
11.053170	799.686521	11.412083
10.974219	781.390796	11.417101
10.908145	776.112736	11.422119
10.637059	778.178079	11.427136
10.472893	779.291909	11.432154
11.202674	785.755447	11.437171
10.696743	802.417981	11.442189
10.764291	803.246997	11.447207
10.885553	809.113711	11.452224
11.015971	814.820258	11.457242
10.956457	807.256177	11.462259
10.885434	803.736711	11.467277
10.894666	808.412590	11.472295
11.072439	800.090752	11.477312
10.656341	807.568025	11.482330
11.025026	800.510175	11.487347
10.946561	810.497155	11.492365
10.714567	809.460518	11.497383
10.769535	805.113143	11.502400
10.915748	811.762300	11.507418
11.205110	807.215094	11.512435
10.984498	809.661040	11.517453
11.053567	807.547436	11.522471
10.953168	814.413801	11.527488
11.008814	809.995055	11.532506
11.109504	801.428120	11.537523
11.327691	802.990421	11.542541
11.300423	798.550765	11.547559
11.036350	802.109362	11.552576
11.283653	818.554665	11.557594
11.518111	802.160856	11.562611
11.486330	812.212937	11.567629
11.305420	806.166127	11.572647
11.162398	808.090589	11.577664
11.133180	811.707536	11.582682
10.961817	806.503984	11.587699
10.881600	806.071710	11.592717
10.931936	808.423184	11.597735
10.786184	809.381612	11.602752
11.359473	805.483811	11.607770
11.140228	802.350289	11.612787
11.157733	808.524327	11.617805
11.120583	804.386684	11.622823
11.085783	811.359108	11.627840
10.970575	829.819867	11.632858
11.554072	830.228423	11.637875
11.164841	832.713318	11.642893
11.221194	833.602062	11.647911
11.302878	825.130776	11.652928
11.217232	830.371558	11.657946
11.602069	828.820985	11.662963
11.158550	838.934572	11.667981
11.100689	831.418235	11.672999
11.120727	822.591429	11.678016
11.418366	828.145887	11.683034
11.357451	824.935750	11.688051
11.320662	831.412868	11.693069
11.291985	838.356732	11.698087
11.442664	827.716646	11.703104
11.550721	828.716506	11.708122
11.275214	828.551203	11.713139
11.158093	831.094970	11.718157
11.469188	829.974304	11.723175
11.769592	831.021442	11.728192
11.050230	833.338969	11.733210
11.553156	828.901661	11.738227
11.624038	827.547952	11.743245
11.623423	824.502624	11.748263
11.646834	821.725746	11.753280
11.291083	826.421914	11.758298
11.570091	820.023362	11.763315
11.388874	829.749824	11.768333
11.566395	853.064649	11.773351
11.814596	849.653720	11.778368
11.788572	850.982463	11.783386
11.457593	832.495353	11.788403
11.357971	845.837268	11.793421
11.663729	850.253043	11.798439
11.823632	858.484522	11.803456
11.743906	862.090948	11.808474
11.907399	852.765589	11.813491
11.797727	841.152120	11.818509
11.523081	836.810108	11.823527
11.278829	836.486487	11.828544
11.634575	851.585981	11.833562
11.509008	854.170125	11.838579
11.416737	862.752405	11.843597
11.339199	861.767349	11.848615
11.573103	856.099839	11.853632
11.399570	863.113763	11.858650
11.746037	857.193372	11.863667
11.560133	860.946901	11.868685
11.527705	858.584362	11.873703
12.040849	864.179127	11.878720
11.668958	864.625031	11.883738
11.647152	867.535286	11.888755
11.801323	888.917508	11.893773
11.848385	894.635525	11.898791
12.135001	889.149424	11.903808
12.118357	902.096167	11.908826
12.038894	879.791931	11.913843
12.046610	880.386383	11.918861
12.049385	872.203717	11.923879
12.127200	871.188997	11.928896
12.101770	869.385901	11.933914
11.994157	861.667562	11.938931
12.136574	860.995278	11.943949
11.899643	862.973091	11.948967
11.985397	856.946274	11.953984
11.754506	859.656909	11.959002
11.515448	861.986238	11.964019
11.667118	868.023128	11.969037
11.963457	885.754023	11.974055
12.230204	889.642829	11.979072
11.862322	906.657793	11.984090
12.393330	896.349937	11.989107
12.052718	896.600908	11.994125
12.126143	893.309458	11.999143
12.252249	878.126371	12.004160
12.129902	868.175533	12.009178
12.191409	861.575591	12.014195
11.808766	862.047684	12.019213
12.220479	876.543475	12.024231
12.382935	886.966964	12.029248
11.998258	890.202654	12.034266
12.227647	880.216790	12.039283
12.597201	887.472667	12.044301
12.275298	875.004594	12.049319
12.311667	862.163044	12.054336
12.086898	861.975167	12.059354
12.231478	856.112616	12.064371
12.192463	861.498828	12.069389
11.812239	864.685353	12.074407
12.226213	866.823871	12.079424
12.249673	881.196566	12.084442
12.530918	880.021394	12.089459
12.701170	879.272063	12.094477
12.153963	872.998889	12.099495
12.592692	851.982441	12.104512
12.031592	858.469231	12.109530
12.198439	858.414132	12.114547
12.387940	859.113120	12.119565
12.395577	882.789176	12.124583
12.385251	875.321243	12.129600
12.166974	883.156720	12.134618
12.489909	885.786279	12.139635
12.496217	885.325894	12.144653
12.230426	883.511027	12.149671
12.430130	885.653535	12.154688
12.712258	893.984473	12.159706
12.545059	880.236897	12.164723
12.464606	875.058818	12.169741
12.359496	880.769747	12.174759
12.384125	887.310336	12.179776
12.359596	893.070521	12.184794
12.420094	891.506725	12.189811
12.490232	890.324780	12.194829
12.357426	895.585203	12.199847
12.164005	891.272637	12.204864
12.340794	893.374455	12.209882
12.470301	888.345058	12.214899
12.648406	886.858634	12.219917
12.466700	895.091979	12.224935
12.332508	888.738202	12.229952
12.329825	893.927867	12.234970
12.146424	883.363142	12.239987
12.263567	896.747942	12.245005
11.983472	917.562775	12.250023
12.228243	918.074668	12.255040
12.532028	921.017627	12.260058
12.709181	927.032998	12.265075
12.653169	921.815030	12.270093
12.555252	935.442553	12.275111
12.687229	930.499345	12.280128
12.869270	923.686905	12.285146
12.672434	929.968529	12.290163
13.076872	925.513253	12.295181
13.009637	930.921878	12.300199
13.002794	929.338128	12.305216
12.847838	929.887869	12.310234
12.744373	926.089902	12.315251
12.826293	923.959587	12.320269
12.598926	936.636937	12.325287
12.848540	921.519965	12.330304
13.121662	929.147326	12.335322
12.751074	933.355847	12.340339
12.967004	923.672171	12.345357
12.952656	932.823057	12.350375
12.893731	932.975810	12.355392
13.090840	929.165468	12.360410
12.905200	926.456258	12.365427
13.134231	925.305083	12.370445
12.762259	936.076541	12.375463
12.764791	929.856792	12.380480
13.015961	930.241254	12.385498
12.853600	933.081492	12.390515
13.061743	931.050349	12.395533
12.844107	936.318141	12.400551
12.715070	938.098970	12.405568
13.136328	927.930128	12.410586
12.992985	930.975476	12.415603
13.469271	922.900584	12.420621
12.916020	927.057858	12.425639
12.986731	923.412931	12.430656
12.946629	930.764222	12.435674
12.652061	933.005120	12.440691
12.834933	934.183142	12.445709
12.939201	953.045085	12.450727
13.087277	949.220418	12.455744
13.268191	953.365570	12.460762
13.011387	956.429317	12.465779
13.378570	953.567931	12.470797
13.218430	960.696998	12.475815
13.201270	961.988851	12.480832
13.144810	960.001520	12.485850
13.113435	953.491720	12.490867
13.420017	947.414914	12.495885
13.047415	957.546361	12.500903
13.080754	949.615275	12.505920
13.058018	949.149856	12.510938
13.264705	954.426913	12.515955
13.505951	948.802246	12.520973
13.505533	958.531919	12.525991
13.754407	948.683330	12.531008
13.530066	953.585718	12.536026
13.559543	956.609145	12.541043
13.758218	941.816324	12.546061
13.414153	934.540629	12.551079
13.509946	923.827680	12.556096
13.218831	920.835163	12.561114
12.975572	928.252771	12.566131
13.452166	934.379969	12.571149
13.345392	951.858415	12.576167
13.738068	949.598688	12.581184
13.786923	949.411953	12.586202
13.393320	939.697318	12.591219
13.384509	933.123556	12.596237
13.337866	944.645050	12.601255
13.590487	950.805013	12.606272
13.364268	954.088489	12.611290
13.456243	957.133062	12.616307
13.582991	943.529266	12.621325
13.455160	955.281919	12.626343
13.606284	950.987081	12.631360
13.693324	948.433492	12.636378
13.346449	954.982875	12.641395
13.281199	955.150455	12.646413
13.474435	952.426530	12.651431
13.440058	945.043645	12.656448
13.501130	944.523405	12.661466
12.974274	954.611499	12.666483
13.633051	961.837626	12.671501
13.584048	974.383113	12.676519
13.720284	975.105493	12.681536
14.031026	985.689132	12.686554
13.665390	970.273616	12.691571
13.790400	970.146315	12.696589
13.118161	978.548332	12.701607
13.228410	980.693069	12.706624
13.747574	982.914968	12.711642
13.344484	981.833820	12.716659
13.524513	982.218253	12.721677
13.586394	983.661973	12.726695
13.569299	984.536510	12.731712
13.941460	992.950620	12.736730
13.789347	997.163923	12.741747
13.876437	995.492567	12.746765
14.178949	1001.325403	12.751783
13.967287	987.334712	12.756800
14.042186	985.000835	12.761818
13.975571	982.453788	12.766835
13.681829	986.628732	12.771853
14.033125	979.457545	12.776871
14.086849	984.012334	12.781888
14.135659	976.877853	12.786906
14.120193	979.748891	12.791923
14.140287	974.345868	12.796941
14.267938	975.001956	12.801959
14.323455	979.390706	12.806976
14.391623	978.962593	12.811994
14.242488	978.027179	12.817011
14.264058	980.273605	12.822029
13.922063	984.528977	12.827047
13.590409	980.771145	12.832064
13.965698	972.644844	12.837082
13.731485	977.196921	12.842099
14.039273	984.921321	12.847117
14.021897	977.929683	12.852135
14.076395	983.226047	12.857152
13.919867	978.502244	12.862170
13.755781	983.317895	12.867187
13.829061	991.089005	12.872205
14.284098	1005.963161	12.877223
14.161463	1005.696560	12.882240
14.212990	1009.115544	12.887258
14.462656	1015.290194	12.892275
14.120048	1008.674041	12.897293
14.212480	1006.244348	12.902311
14.216968	1006.627930	12.907328
14.404867	1008.482264	12.912346
14.219241	1011.490930	12.917363
14.505046	1009.470931	12.922381
14.443546	1011.291764	12.927399
14.299864	1015.806026	12.932416
14.373585	1011.111406	12.937434
14.369501	1014.595503	12.942451
14.322955	1010.023945	12.947469
14.259799	1013.397750	12.952487
14.183462	1013.780937	12.957504
14.821418	1007.275233	12.962522
14.574774	1015.032406	12.967539
14.418838	1008.774302	12.972557
14.784222	1008.004857	12.977575
14.532026	1020.347817	12.982592
14.510304	1014.839504	12.987610
14.418976	1022.627652	12.992627
14.415168	1006.241589	12.997645
14.508545	1015.774276	13.002663
14.693208	1012.008100	13.007680
14.660066	1007.218977	13.012698
14.279450	1017.687209	13.017715
14.592972	1011.941894	13.022733
14.670280	1005.957755	13.027751
14.386207	1006.325738	13.032768
14.559971	1007.272604	13.037786
14.451462	1016.218275	13.042803
14.330875	1008.702003	13.047821
14.675135	1007.729370	13.052839
14.545312	1018.672196	13.057856
14.870148	1025.443829	13.062874
14.716513	1030.687276	13.067891
14.755542	1028.166033	13.072909
14.496706	1028.564875	13.077927
14.643328	1035.557355	13.082944
14.765705	1046.756458	13.087962
14.788129	1046.433159	13.092979
15.070252	1048.717942	13.097997
14.953751	1036.923574	13.103015
15.082988	1040.279698	13.108032
15.010081	1026.216783	13.113050
14.859333	1024.214744	13.118067
14.530743	1015.492801	13.123085
15.077740	1027.532566	13.128103
15.026498	1037.410069	13.133120
15.235640	1028.447504	13.138138
14.848099	1017.196440	13.143155
14.850129	1000.894845	13.148173
14.630586	1004.903183	13.153191
15.232583	1031.515573	13.158208
14.943087	1021.601370	13.163226
14.845503	1035.679697	13.168243
14.927057	1036.017842	13.173261
15.283319	1046.202266	13.178279
14.943042	1037.964906	13.183296
15.168493	1046.707660	13.188314
15.064717	1047.524116	13.193331
15.073322	1041.669446	13.198349
15.138410	1035.066082	13.203367
14.901788	1044.222346	13.208384
15.332250	1044.033439	13.213402
14.929041	1045.997866	13.218419
14.987281	1044.985984	13.223437
14.918333	1046.611211	13.228455
15.252771	1038.516050	13.233472
15.181004	1045.049440	13.238490
15.210163	1041.219641	13.243507
15.064910	1049.070273	13.248525
15.342091	1048.639436	13.253543
14.814850	1052.284973	13.258560
15.113451	1049.056593	13.263578
15.051897	1044.899700	13.268595
14.720412	1049.493495	13.273613
14.945969	1052.972249	13.278631
14.860134	1069.976905	13.283648
15.147730	1073.217839	13.288666
15.102800	1081.186909	13.293683
15.208050	1077.194899	13.298701
15.181846	1078.795729	13.303719
14.964722	1083.603659	13.308736
14.920818	1078.854877	13.313754
15.248161	1097.456442	13.318771
15.002293	1110.097234	13.323789
15.230055	1099.073343	13.328807
15.292615	1112.245328	13.333824
15.502224	1100.661468	13.338842
15.744820	1106.070815	13.343859
15.463434	1114.802657	13.348877
15.769891	1105.732598	13.353895
15.630922	1109.483139	13.358912
15.661168	1105.281895	13.363930
15.728617	1102.116584	13.368947
15.903368	1106.036821	13.373965
15.782795	1111.254348	13.378983
15.654765	1122.030419	13.384000
15.717569	1101.027856	13.389018
15.936065	1111.379226	13.394035
15.808249	1106.204188	13.399053
16.261528	1096.962188	13.404071
15.664962	1088.281036	13.409088
15.683573	1074.600548	13.414106
15.633560	1068.903207	13.419123
15.779126	1079.729215	13.424141
16.008552	1070.013293	13.429159
15.666675	1073.764750	13.434176
15.790152	1071.816110	13.439194
15.899398	1073.570488	13.444211
15.609222	1077.761007	13.449229
16.099600	1064.289798	13.454247
15.860554	1074.565734	13.459264
16.166558	1070.329071	13.464282
15.951404	1073.106426	13.469299
15.440136	1070.407414	13.474317
15.646267	1077.169593	13.479335
15.759854	1086.697403	13.484352
15.831975	1099.415840	13.489370
16.052595	1101.766326	13.494387
15.886390	1105.006038	13.499405
15.751826	1103.994584	13.504423
15.806742	1108.976364	13.509440
15.942397	1109.625227	13.514458
16.043139	1106.724472	13.519475
15.680653	1114.276475	13.524493
15.695570	1100.452485	13.529511
15.777771	1104.595914	13.534528
15.354382	1101.415036	13.539546
15.783607	1119.687562	13.544563
15.656030	1127.224686	13.549581
16.293120	1128.099955	13.554599
16.097168	1133.993337	13.559616
16.240405	1133.040994	13.564634
16.597058	1133.388703	13.569651
16.234777	1135.842805	13.574669
16.346510	1125.538876	13.579687
16.134800	1138.085848	13.584704
16.196316	1133.068419	13.589722
16.315727	1128.989407	13.594739
16.099495	1134.675918	13.599757
16.231793	1127.653917	13.604775
16.135350	1144.785604	13.609792
16.534077	1133.686923	13.614810
16.561793	1135.870545	13.619827
16.535558	1143.576717	13.624845
16.787813	1131.483031	13.629863
16.253388	1136.758468	13.634880
16.286657	1138.821095	13.639898
16.276892	1141.345166	13.644915
16.245114	1143.418959	13.649933
16.598962	1125.692086	13.654951
16.302768	1126.240812	13.659968
16.349290	1137.562775	13.664986
16.700216	1136.381557	13.670003
16.335928	1139.964305	13.675021
16.656450	1135.737032	13.680039
16.545874	1132.505135	13.685056
16.260763	1132.844946	13.690074
16.425372	1132.678016	13.695091
15.979568	1128.696931	13.700109
16.129913	1120.162936	13.705127
16.388729	1133.526449	13.710144
16.252514	1154.152423	13.715162
16.661424	1157.283919	13.720179
16.445617	1172.850015	13.725197
16.437158	1159.363693	13.730215
16.749081	1160.512094	13.735232
16.496373	1157.999378	13.740250
16.601929	1160.880329	13.745267
16.848807	1171.285306	13.750285
17.082590	1161.029644	13.755303
16.938358	1171.795835	13.760320
16.905449	1166.013738	13.765338
16.924884	1153.955045	13.770355
16.643832	1167.280430	13.775373
16.895654	1162.540919	13.780391
17.265766	1162.908053	13.785408
16.862204	1160.296698	13.790426
16.903112	1154.930716	13.795443
16.656334	1159.697911	13.800461
16.682052	1148.963341	13.805479
16.923668	1155.540550	13.810496
16.918512	1156.822558	13.815514
17.223598	1157.488247	13.820531
16.927796	1170.198378	13.825549
17.097825	1157.355317	13.830567
16.964179	1167.709134	13.835584
16.767271	1165.802907	13.840602
17.174616	1162.377368	13.845619
16.827342	1158.357519	13.850637
17.105112	1154.486523	13.855655
17.333129	1160.938824	13.860672
17.297559	1163.016398	13.865690
17.155490	1149.775824	13.870707
17.247450	1158.269101	13.875725
17.261336	1159.720785	13.880743
16.988171	1152.803708	13.885760
17.160162	1158.992460	13.890778
17.348474	1146.513693	13.895795
17.065320	1162.703906	13.900813
16.996560	1162.448065	13.905831
17.161519	1173.232346	13.910848
17.205343	1161.215276	13.915866
17.450828	1158.423611	13.920883
17.036601	1159.533995	13.925901
16.841855	1158.816353	13.930919
17.440760	1162.380548	13.935936
16.959049	1159.539621	13.940954
17.328318	1164.374091	13.945971
17.232474	1183.785579	13.950989
17.399927	1180.587551	13.956007
17.652528	1186.788162	13.961024
17.523893	1192.099962	13.966042
17.524761	1179.151828	13.971059
17.432263	1178.505833	13.976077
17.418891	1180.754531	13.981095
17.598052	1187.562169	13.986112
17.546543	1186.681440	13.991130
17.633939	1180.084556	13.996147
17.089755	1176.542573	14.001165
17.470817	1182.644353	14.006183
17.660586	1184.223209	14.011200
17.170416	1192.603458	14.016218
17.533982	1186.624995	14.021235
17.285439	1180.990408	14.026253
17.152892	1193.505419	14.031271
17.272055	1181.829392	14.036288
17.497437	1184.621609	14.041306
17.540911	1202.795123	14.046323
17.533335	1211.251763	14.051341
17.569773	1220.632198	14.056359
17.704442	1223.732351	14.061376
17.469650	1229.791646	14.066394
17.898764	1212.521097	14.071411
17.629419	1219.905762	14.076429
17.553633	1228.062296	14.081447
17.892569	1216.668740	14.086464
17.899313	1227.347765	14.091482
18.015326	1212.473102	14.096499
17.707462	1213.478870	14.101517
17.846365	1215.585825	14.106535
17.982995	1202.641961	14.111552
17.832341	1220.585444	14.116570
18.083238	1215.655129	14.121587
17.979507	1214.168889	14.126605
17.893427	1208.899505	14.131623
18.125850	1215.057013	14.136640
17.659570	1216.261058	14.141658
18.103248	1213.281449	14.146675
17.705498	1220.039362	14.151693
17.907566	1218.610353	14.156711
18.334362	1232.599269	14.161728
17.882603	1229.341174	14.166746
18.480974	1231.806288	14.171763
18.376186	1227.136439	14.176781
18.204112	1222.043098	14.181799
18.228850	1226.826375	14.186816
18.222456	1218.502922	14.191834
18.022914	1210.059098	14.196851
18.115496	1221.437667	14.201869
18.248329	1219.667770	14.206887
18.418251	1209.540365	14.211904
18.174940	1217.023865	14.216922
18.372224	1212.958707	14.221939
18.351610	1214.698780	14.226957
18.085187	1216.060669	14.231975
18.362822	1230.256562	14.236992
18.312203	1247.800056	14.242010
18.719594	1241.121023	14.247027
18.626051	1231.214788	14.252045
18.328993	1230.197950	14.257063
18.306991	1217.138220	14.262080
18.369445	1229.198144	14.267098
18.430937	1238.249252	14.272115
18.754413	1242.310246	14.277133
18.618871	1238.950968	14.282151
18.648338	1219.346252	14.287168
18.781520	1222.469879	14.292186
18.925862	1209.959760	14.297203
18.834183	1217.958689	14.302221
18.583427	1220.456932	14.307239
18.532622	1203.838685	14.312256
18.362130	1214.845074	14.317274
18.373627	1218.003810	14.322291
18.502481	1211.419338	14.327309
18.094198	1237.005707	14.332327
18.683282	1234.408699	14.337344
18.555547	1250.793734	14.342362
18.821779	1247.504927	14.347379
18.969050	1242.996086	14.352397
19.056983	1248.980688	14.357415
18.802047	1246.967920	14.362432
18.614253	1252.616695	14.367450
18.859780	1240.834267	14.372467
18.952707	1249.776636	14.377485
18.723123	1253.363874	14.382503
19.234724	1245.383754	14.387520
19.352388	1249.696149	14.392538
19.304243	1232.235717	14.397555
19.129475	1218.784757	14.402573
18.831668	1220.814032	14.407591
19.007919	1205.882550	14.412608
18.776154	1207.352083	14.417626
18.654932	1221.842357	14.422643
19.087754	1234.676761	14.427661
18.947384	1247.880497	14.432679
19.167247	1238.947138	14.437696
19.250963	1239.521145	14.442714
19.196781	1230.251684	14.447731
19.083821	1242.748137	14.452749
19.093995	1242.488672	14.457767
19.198022	1229.829311	14.462784
18.946375	1244.521120	14.467802
18.981598	1237.563568	14.472819
19.336376	1231.510561	14.477837
19.071491	1231.496639	14.482855
19.133626	1237.980773	14.487872
19.124725	1245.255001	14.492890
19.219062	1236.753838	14.497907
19.324807	1234.248285	14.502925
19.277648	1241.446565	14.507943
19.487188	1237.629759	14.512960
19.272217	1239.484694	14.517978
18.855431	1234.579506	14.522995
19.212840	1233.151938	14.528013
18.900716	1240.608656	14.533031
18.995446	1250.008195	14.538048
19.232043	1262.919604	14.543066
19.460773	1270.211186	14.548083
19.512388	1274.456574	14.553101
19.247652	1283.463700	14.558119
19.366635	1270.150662	14.563136
19.560115	1268.660475	14.568154
19.289674	1272.280860	14.573171
19.742420	1274.064599	14.578189
19.435979	1277.055920	14.583207
19.930009	1269.549161	14.588224
19.736910	1274.303565	14.593242
19.819242	1269.959009	14.598259
19.658816	1271.772632	14.603277
19.844810	1273.971795	14.608295
19.881102	1266.350681	14.613312
19.780303	1268.393795	14.618330
19.411281	1273.078908	14.623347
19.642160	1270.098701	14.628365
19.455502	1267.963602	14.633383
19.548390	1268.674671	14.638400
19.494894	1273.672882	14.643418
19.553470	1271.198755	14.648435
20.082824	1279.377154	14.653453
19.909598	1272.837955	14.658471
19.851170	1274.783897	14.663488
19.938530	1273.665212	14.668506
19.817177	1283.568260	14.673523
20.024610	1288.366972	14.678541
19.786449	1291.871388	14.683559
19.929076	1291.528967	14.688576
19.795979	1288.928707	14.693594
19.744303	1296.591137	14.698611
20.303602	1286.509832	14.703629
19.812618	1297.067786	14.708647
20.282765	1291.306275	14.713664
20.084077	1286.349207	14.718682
19.841659	1296.941983	14.723699
20.418295	1293.122642	14.728717
20.054743	1293.664025	14.733735
20.023635	1290.574837	14.738752
20.255972	1294.953687	14.743770
20.056782	1293.626944	14.748787
20.345150	1294.435956	14.753805
20.055613	1289.992740	14.758823
19.864925	1293.963303	14.763840
20.069187	1292.084721	14.768858
19.963618	1304.542992	14.773875
20.408650	1307.813417	14.778893
20.589630	1318.885299	14.783911
20.834674	1309.115068	14.788928
20.980698	1296.292797	14.793946
20.459690	1301.629845	14.798963
20.689780	1282.624493	14.803981
20.492882	1281.971767	14.808999
20.259789	1282.262023	14.814016
20.255630	1283.626945	14.819034
20.457729	1282.474298	14.824051
20.590932	1286.843578	14.829069
20.299115	1284.896753	14.834087
20.507950	1277.366745	14.839104
20.285382	1289.136913	14.844122
20.132404	1312.193383	14.849139
20.628716	1307.291691	14.854157
20.565698	1312.047400	14.859175
20.939138	1319.503621	14.864192
21.065936	1319.864596	14.869210
20.959789	1320.760985	14.874227
21.145394	1312.389153	14.879245
20.745812	1298.950154	14.884263
20.744630	1287.832154	14.889280
20.702590	1296.203997	14.894298
20.458895	1288.319007	14.899315
20.553906	1301.759395	14.904333
20.642133	1320.056736	14.909351
20.675384	1320.552883	14.914368
20.960737	1319.552980	14.919386
20.770334	1320.858590	14.924403
21.235816	1324.082326	14.929421
20.702247	1321.979863	14.934439
20.923656	1315.170970	14.939456
20.958715	1316.117991	14.944474
20.675207	1312.742648	14.949491
21.152986	1314.237212	14.954509
20.945185	1321.809762	14.959527
20.521140	1317.691956	14.964544
20.879552	1326.229783	14.969562
20.813204	1334.755669	14.974579
20.703727	1336.232129	14.979597
20.760716	1343.496279	14.984615
20.988803	1343.153878	14.989632
21.643179	1332.858378	14.994650
21.143880	1338.149718	14.999667
21.743640	1335.976510	15.004685
21.721694	1344.837564	15.009703
21.798757	1341.143456	15.014720
21.876810	1318.087321	15.019738
21.322051	1313.006533	15.024755
21.451694	1301.722768	15.029773
21.239778	1302.454785	15.034791
21.375413	1295.166019	15.039808
21.550673	1294.178443	15.044826
21.498993	1304.398307	15.049843
21.407938	1304.112691	15.054861
21.349007	1303.314286	15.059879
21.398725	1302.778986	15.064896
21.629367	1298.885838	15.069914
21.295444	1309.705188	15.074931
21.549592	1297.303979	15.079949
21.412056	1319.606737	15.084967
21.624788	1323.076653	15.089984
21.825032	1322.185724	15.095002
21.465656	1323.411442	15.100019
22.053454	1324.694486	15.105037
21.566380	1319.435168	15.110055
21.756554	1314.665662	15.115072
21.703252	1301.509471	15.120090
21.514651	1313.797645	15.125107
21.483055	1326.437775	15.130125
21.770456	1334.136200	15.135143
21.694342	1337.684658	15.140160
21.670454	1325.569227	15.145178
21.975321	1331.681321	15.150195
21.716192	1325.173253	15.155213
21.883957	1336.815436	15.160231
21.649814	1332.315004	15.165248
22.220597	1339.924774	15.170266
22.199839	1331.677653	15.175283
21.862906	1339.400726	15.180301
21.842536	1343.004915	15.185319
21.995913	1339.452104	15.190336
22.262720	1340.084378	15.195354
22.031386	1342.490056	15.200371
22.175887	1337.716296	15.205389
22.129534	1339.545288	15.210407
22.205345	1335.834460	15.215424
22.248474	1338.267522	15.220442
22.044623	1343.680410	15.225459
22.035205	1326.543375	15.230477
22.062105	1338.257310	15.235495
22.146594	1339.576062	15.240512
22.101388	1341.582421	15.245530
21.998891	1338.540871	15.250547
21.965146	1335.619038	15.255565
22.021965	1331.980252	15.260583
21.844725	1339.172559	15.265600
22.450782	1344.047009	15.270618
22.353357	1366.489252	15.275635
22.397602	1364.679285	15.280653
22.689807	1364.145167	15.285671
22.450808	1360.941968	15.290688
22.512479	1329.539448	15.295706
22.466661	1336.299368	15.300723
22.485337	1336.553446	15.305741
22.255498	1335.417598	15.310759
22.733015	1356.451258	15.315776
22.860614	1354.325132	15.320794
22.865458	1343.962775	15.325811
22.641717	1331.035566	15.330829
22.777565	1325.339636	15.335847
22.461990	1325.897483	15.340864
22.666917	1319.187773	15.345882
22.502222	1324.275672	15.350899
22.686339	1327.090103	15.355917
22.766218	1345.281771	15.360935
22.404854	1353.343930	15.365952
22.773240	1354.431030	15.370970
22.871618	1349.377506	15.375987
22.736438	1350.886569	15.381005
22.623990	1348.570276	15.386023
22.412504	1355.665507	15.391040
22.786549	1346.264831	15.396058
22.863136	1358.599676	15.401075
23.236633	1353.539964	15.406093
23.251777	1349.578159	15.411111
22.908219	1351.709513	15.416128
23.197811	1349.075468	15.421146
23.368105	1350.511900	15.426163
23.486677	1352.814364	15.431181
23.676943	1346.314546	15.436199
23.002276	1333.141144	15.441216
23.299635	1318.101706	15.446234
23.093079	1323.784715	15.451251
23.121845	1313.535738	15.456269
23.582631	1315.911053	15.461287
23.359041	1307.218013	15.466304
22.891056	1308.749899	15.471322
23.035800	1313.814506	15.476339
23.162722	1327.385064	15.481357
23.628370	1342.486918	15.486375
23.033961	1341.661041	15.491392
23.056390	1339.099584	15.496410
23.015414	1343.944566	15.501427
23.070317	1353.733041	15.506445
23.215328	1346.593877	15.511463
23.043352	1354.738847	15.516480
23.307146	1350.690593	15.521498
23.109218	1357.651692	15.526515
23.274615	1341.630556	15.531533
23.447571	1357.850166	15.536551
23.400069	1374.814163	15.541568
23.643762	1372.838493	15.546586
23.819003	1376.026838	15.551603
23.648569	1371.949303	15.556621
23.506435	1358.797537	15.561639
23.494205	1369.203428	15.566656
23.508438	1369.810992	15.571674
23.754869	1375.167438	15.576691
23.683388	1375.840770	15.581709
23.420330	1374.324993	15.586727
23.569461	1382.629794	15.591744
23.686447	1376.173200	15.596762
23.619630	1367.865971	15.601779
23.696207	1380.855157	15.606797
23.492347	1367.781320	15.611815
23.865561	1373.995105	15.616832
23.795660	1377.377191	15.621850
23.574077	1381.908396	15.626867
23.450041	1385.667947	15.631885
24.273705	1394.763013	15.636903
24.319312	1407.794752	15.641920
24.414117	1393.165156	15.646938
24.194466	1379.777786	15.651955
23.973505	1367.100477	15.656973
24.270300	1365.676636	15.661991
23.721312	1371.293927	15.667008
23.958775	1371.422013	15.672026
24.393135	1383.223232	15.677043
24.228514	1383.093102	15.682061
24.278705	1374.825942	15.687079
23.730406	1379.719116	15.692096
24.186083	1389.519988	15.697114
24.562268	1393.786071	15.702131
24.347932	1406.151807	15.707149
24.488451	1397.207874	15.712167
24.689110	1401.115235	15.717184
24.318325	1381.665568	15.722202
23.922979	1389.544793	15.727219
24.374727	1400.195523	15.732237
24.683963	1398.101124	15.737255
24.790068	1408.131151	15.742272
24.987207	1387.553194	15.747290
24.668539	1384.019487	15.752307
24.497832	1365.043789	15.757325
24.978250	1363.990716	15.762343
24.554571	1366.479035	15.767360
24.450987	1360.616838	15.772378
24.513038	1361.809389	15.777395
24.417116	1364.430832	15.782413
24.568201	1363.080332	15.787431
24.675682	1380.274178	15.792448
24.549782	1379.840397	15.797466
24.764234	1384.217509	15.802483
24.633631	1399.202014	15.807501
24.962650	1391.690632	15.812519
24.961783	1390.302299	15.817536
24.751253	1387.650672	15.822554
25.234663	1397.693410	15.827571
24.957966	1398.499543	15.832589
25.118970	1393.601381	15.837607
24.519383	1381.796588	15.842624
24.703565	1391.532578	15.847642
24.774190	1390.578858	15.852659
24.777961	1396.512887	15.857677
25.019999	1388.754102	15.862695
24.992212	1384.141139	15.867712
24.962301	1390.398456	15.872730
24.924478	1396.206304	15.877747
24.756686	1398.966425	15.882765
25.098201	1382.410184	15.887783
25.209863	1392.632586	15.892800
25.021744	1389.353240	15.897818
25.152945	1387.991463	15.902835
24.925193	1391.501264	15.907853
25.175539	1403.207381	15.912871
25.289629	1419.958451	15.917888
25.468317	1422.711201	15.922906
25.632696	1416.528235	15.927923
25.380830	1411.762214	15.932941
25.535281	1394.468836	15.937959
25.239401	1399.143843	15.942976
25.173184	1408.265410	15.947994
25.660304	1411.094642	15.953011
25.500313	1425.474991	15.958029
25.620336	1414.419112	15.963047
25.533829	1425.738511	15.968064
25.642393	1415.778218	15.973082
25.605241	1423.758380	15.978099
25.665120	1418.194680	15.983117
25.446036	1408.252427	15.988135
25.122514	1422.595681	15.993152
25.442466	1416.865295	15.998170
25.731990	1416.894211	16.003187
25.675624	1417.467799	16.008205
25.691398	1418.771559	16.013223
25.109244	1413.877948	16.018240
25.175154	1418.950526	16.023258
25.366721	1435.359259	16.028275
25.200641	1451.470937	16.033293
25.684266	1446.678782	16.038311
25.980499	1441.964116	16.043328
25.745034	1442.328388	16.048346
25.918768	1444.136697	16.053363
26.018271	1441.687262	16.058381
26.320303	1439.348383	16.063399
25.995376	1446.890389	16.068416
25.855255	1449.502631	16.073434
26.115507	1442.056548	16.078451
25.885716	1444.827337	16.083469
26.164819	1452.193733	16.088487
26.307292	1469.473616	16.093504
26.606550	1463.367903	16.098522
26.560323	1449.375776	16.103539
26.110149	1442.567013	16.108557
26.718900	1437.321468	16.113575
26.490426	1451.011614	16.118592
26.626386	1441.164483	16.123610
26.425461	1436.237658	16.128627
26.303846	1436.644495	16.133645
26.378386	1438.210175	16.138663
26.422586	1429.612485	16.143680
26.530310	1432.726985	16.148698
26.551923	1434.911659	16.153715
26.582113	1439.568116	16.158733
26.626004	1438.615277	16.163751
26.645063	1440.203924	16.168768
26.862905	1434.665242	16.173786
27.396901	1428.989564	16.178803
26.862802	1440.100023	16.183821
26.645024	1431.842167	16.188839
26.755926	1437.956502	16.193856
26.805257	1434.979555	16.198874
26.912135	1432.997005	16.203891
26.575370	1442.048040	16.208909
26.894236	1430.630880	16.213927
26.936867	1429.674313	16.218944
26.735639	1438.121411	16.223962
27.053478	1423.159189	16.228979
26.445282	1435.868511	16.233997
26.709268	1427.709225	16.239015
26.757208	1440.715015	16.244032
26.588809	1440.882750	16.249050
26.991740	1431.264250	16.254067
26.866136	1439.947249	16.259085
26.942034	1439.934769	16.264103
26.754988	1441.246919	16.269120
26.895125	1449.309941	16.274138
27.018157	1441.031865	16.279155
26.833327	1443.928278	16.284173
26.735115	1455.760262	16.289191
26.877197	1461.513935	16.294208
26.996284	1466.708430	16.299226
27.298367	1465.730551	16.304243
27.343693	1459.255869	16.309261
27.310298	1462.179964	16.314279
27.193444	1465.260399	16.319296
27.098079	1466.717604	16.324314
27.237454	1459.669085	16.329331
27.143505	1464.403979	16.334349
27.337845	1469.597038	16.339367
27.588395	1454.369159	16.344384
27.441993	1460.755635	16.349402
27.597228	1459.659161	16.354419
27.476396	1467.807926	16.359437
27.765169	1473.284953	16.364455
27.992921	1467.723752	16.369472
27.603278	1467.904502	16.374490
27.640285	1462.552445	16.379507
27.491356	1463.838601	16.384525
27.415987	1466.094850	16.389543
27.923354	1476.049815	16.394560
27.692485	1485.712074	16.399578
27.680963	1491.377021	16.404595
27.740706	1489.848723	16.409613
27.819687	1485.803085	16.414631
28.096605	1478.304619	16.419648
28.117100	1485.691414	16.424666
28.371624	1481.507654	16.429683
28.049409	1468.189159	16.434701
28.075166	1460.426783	16.439719
28.417672	1450.990321	16.444736
28.028059	1451.603739	16.449754
27.853136	1451.130829	16.454771
27.927594	1448.515857	16.459789
28.349680	1453.254666	16.464807
28.145933	1450.207814	16.469824
27.994330	1458.413637	16.474842
28.288990	1444.607584	16.479859
28.083540	1450.040065	16.484877
27.858979	1466.411046	16.489895
28.606029	1481.746359	16.494912
28.096036	1488.698562	16.499930
28.399868	1486.828666	16.504947
28.363073	1482.147087	16.509965
28.095851	1479.115071	16.514983
28.560836	1473.713007	16.520000
28.495046	1472.776753	16.525018
28.596805	1472.493458	16.530035
28.366976	1483.927576	16.535053
28.365441	1482.910997	16.540071
28.603782	1478.688973	16.545088
28.378123	1480.615783	16.550106
28.795407	1472.697623	16.555123
28.594483	1475.100254	16.560141
28.426111	1476.501834	16.565159
28.431183	1475.521562	16.570176
28.271039	1475.778875	16.575194
28.706434	1472.632088	16.580211
28.659363	1475.387192	16.585229
28.411924	1480.174673	16.590247
28.895611	1477.055320	16.595264
29.031582	1499.407534	16.600282
29.039793	1499.094453	16.605299
28.892417	1479.367119	16.610317
28.566746	1486.113210	16.615335
28.921749	1493.305248	16.620352
28.959508	1505.312785	16.625370
29.347936	1502.048179	16.630387
29.291948	1499.176848	16.635405
29.171546	1492.800066	16.640423
29.012497	1489.482026	16.645440
29.009638	1499.403386	16.650458
29.262374	1502.555304	16.655475
29.205941	1495.733679	16.660493
29.193552	1503.828679	16.665511
29.414845	1501.198832	16.670528
29.331676	1504.746922	16.675546
29.401934	1504.509393	16.680563
29.220989	1501.357574	16.685581
28.798972	1497.005526	16.690599
29.532923	1495.675425	16.695616
29.271083	1498.996408	16.700634
29.293873	1504.182453	16.705651
29.337325	1503.736372	16.710669
29.435768	1501.459937	16.715687
29.435479	1501.108107	16.720704
29.282078	1498.801328	16.725722
29.348617	1493.196341	16.730739
29.501301	1486.718043	16.735757
29.294398	1509.500667	16.740775
29.443745	1521.154306	16.745792
29.776000	1529.963900	16.750810
29.675301	1527.061778	16.755827
29.964803	1530.802493	16.760845
29.602452	1525.825598	16.765863
30.017983	1518.654946	16.770880
30.190533	1515.246952	16.775898
30.235758	1514.348217	16.780915
30.173924	1508.693616	16.785933
30.128052	1509.311927	16.790951
30.117895	1486.915419	16.795968
30.056997	1474.260335	16.800986
29.919683	1480.588229	16.806003
29.988517	1483.307606	16.811021
29.944323	1502.434959	16.816039
30.562189	1495.040656	16.821056
30.385232	1501.472760	16.826074
29.984945	1479.501099	16.831091
30.095873	1479.039515	16.836109
29.929408	1510.718920	16.841127
30.463913	1501.575043	16.846144
30.242260	1508.112582	16.851162
30.340006	1504.181941	16.856179
30.437973	1508.049247	16.861197
30.353770	1507.741233	16.866215
30.404187	1503.919216	16.871232
30.476556	1502.239221	16.876250
30.314902	1506.375107	16.881267
30.632566	1505.880470	16.886285
30.433252	1510.624558	16.891303
30.757725	1507.785499	16.896320
30.442964	1516.176637	16.901338
30.443985	1506.344723	16.906355
30.350643	1504.255556	16.911373
30.450735	1509.210300	16.916391
30.635413	1507.998318	16.921408
30.497546	1511.816095	16.926426
30.525098	1514.888768	16.931443
30.601109	1512.793604	16.936461
30.518582	1518.877404	16.941479
31.058859	1527.302945	16.946496
31.077701	1540.064818	16.951514
30.537636	1528.303206	16.956531
31.018676	1535.583054	16.961549
30.779618	1535.480209	16.966567
30.709607	1530.095063	16.971584
30.866290	1548.496692	16.976602
30.635090	1546.374442	16.981619
31.177723	1539.111867	16.986637
30.936458	1537.089316	16.991655
30.920714	1536.233353	16.996672
31.156587	1534.640059	17.001690
31.115535	1533.696162	17.006707
31.211523	1531.154775	17.011725
31.010811	1538.653028	17.016743
31.361420	1549.002895	17.021760
31.747097	1550.073367	17.026778
31.555267	1541.243834	17.031795
32.022359	1523.573346	17.036813
31.383814	1531.050002	17.041831
31.655191	1535.944108	17.046848
31.405547	1528.116672	17.051866
31.595441	1528.572714	17.056883
31.879478	1528.000181	17.061901
31.212463	1533.004005	17.066919
31.504446	1526.131365	17.071936
31.481540	1520.021103	17.076954
31.396533	1522.843915	17.081971
31.154986	1533.846941	17.086989
31.509874	1546.324041	17.092007
32.081293	1553.976333	17.097024
32.036653	1556.236169	17.102042
31.913288	1557.853137	17.107059
32.195614	1555.408056	17.112077
32.177209	1555.873789	17.117095
31.948833	1544.844800	17.122112
32.070394	1542.468075	17.127130
32.070226	1532.683585	17.132147
32.107275	1528.544879	17.137165
31.960653	1528.721608	17.142183
32.228122	1537.464375	17.147200
32.119508	1535.708046	17.152218
31.885956	1538.104279	17.157235
31.951423	1549.435217	17.162253
32.137447	1548.897023	17.167271
32.285669	1544.877698	17.172288
32.002930	1557.531258	17.177306
31.875492	1556.868198	17.182323
32.284115	1555.388816	17.187341
31.971399	1555.413521	17.192359
32.084652	1552.388565	17.197376
32.138405	1554.515966	17.202394
32.157200	1565.276693	17.207411
32.664157	1569.815659	17.212429
32.402404	1578.419706	17.217447
32.398088	1570.615010	17.222464
32.885339	1577.741882	17.227482
32.536850	1582.052033	17.232499
33.248818	1571.793297	17.237517
33.234571	1581.585886	17.242535
33.040955	1550.103932	17.247552
32.672990	1552.346441	17.252570
32.390957	1552.927087	17.257587
32.670272	1542.447101	17.262605
32.584396	1558.227499	17.267623
32.927119	1564.263340	17.272640
33.087676	1570.578167	17.277658
32.978831	1572.520290	17.282675
32.967940	1569.256046	17.287693
32.990601	1581.654724	17.292711
32.932179	1574.017253	17.297728
33.244401	1567.900298	17.302746
33.206801	1579.427458	17.307763
33.232688	1569.078001	17.312781
33.090349	1568.981581	17.317799
32.933332	1568.162789	17.322816
33.288649	1571.223719	17.327834
33.039046	1567.957271	17.332851
33.359771	1560.597968	17.337869
33.127643	1574.230166	17.342887
33.102637	1563.326937	17.347904
33.465149	1562.186290	17.352922
33.066146	1570.151250	17.357939
33.461275	1568.071346	17.362957
33.245193	1566.002495	17.367975
33.164565	1561.232481	17.372992
33.340412	1574.044369	17.378010
33.348069	1589.241989	17.383027
33.705862	1592.062750	17.388045
33.717038	1605.117678	17.393063
33.820868	1601.221832	17.398080
33.794325	1601.577497	17.403098
33.615801	1609.581558	17.408115
33.933771	1599.541196	17.413133
33.595070	1609.111938	17.418151
33.686020	1601.128066	17.423168
33.815137	1602.614648	17.428186
33.857646	1604.715571	17.433203
34.210247	1599.137587	17.438221
34.184905	1602.457619	17.443239
33.903899	1600.840853	17.448256
34.072045	1602.037901	17.453274
34.036449	1606.861207	17.458291
33.863237	1600.436826	17.463309
34.062499	1605.201557	17.468327
33.707786	1600.439909	17.473344
34.295124	1599.931322	17.478362
34.052066	1606.361029	17.483379
34.167923	1601.784845	17.488397
34.232749	1595.587585	17.493415
34.594988	1614.637932	17.498432
34.659794	1605.602086	17.503450
34.409143	1611.096044	17.508467
34.411327	1596.311516	17.513485
34.444071	1605.873505	17.518503
34.350243	1601.326924	17.523520
34.795906	1602.422113	17.528538
34.481116	1605.583776	17.533555
34.836760	1610.228125	17.538573
34.966796	1606.335419	17.543591
34.958664	1600.166380	17.548608
34.770172	1586.910284	17.553626
34.607833	1585.062059	17.558643
34.766044	1585.366657	17.563661
34.907856	1582.928304	17.568679
34.953187	1596.860247	17.573696
35.157590	1586.183187	17.578714
34.680403	1589.489061	17.583731
35.077108	1587.259287	17.588749
34.964304	1592.167421	17.593767
34.710246	1583.367066	17.598784
34.693254	1593.331771	17.603802
34.669693	1606.710956	17.608819
34.795577	1603.209096	17.613837
35.071603	1609.520566	17.618855
34.898900	1616.038627	17.623872
35.381647	1611.341451	17.628890
35.371345	1613.243246	17.633907
35.474281	1609.586129	17.638925
35.348079	1619.644131	17.643943
34.974631	1616.313535	17.648960
35.332355	1610.313832	17.653978
34.924334	1623.005119	17.658995
35.233471	1605.461482	17.664013
35.588131	1614.629619	17.669031
35.352747	1630.160832	17.674048
35.419203	1644.618848	17.679066
35.706499	1643.104036	17.684083
35.681227	1644.722880	17.689101
35.685989	1643.256033	17.694119
35.577140	1645.680452	17.699136
35.979774	1637.818965	17.704154
36.071724	1643.791638	17.709171
36.132159	1641.219507	17.714189
35.654108	1631.157393	17.719207
35.579187	1644.371100	17.724224
35.764301	1628.314908	17.729242
36.013339	1644.899387	17.734259
35.699038	1639.023157	17.739277
36.119056	1640.385588	17.744295
35.753394	1638.971419	17.749312
35.712147	1641.829919	17.754330
36.072847	1638.180506	17.759347
35.861092	1635.929826	17.764365
35.975087	1639.120101	17.769383
36.106441	1655.398487	17.774400
36.074848	1670.423158	17.779418
36.215719	1662.236499	17.784435
36.088534	1659.588739	17.789453
36.434001	1661.638323	17.794471
36.385389	1660.345274	17.799488
36.824368	1646.537586	17.804506
36.453461	1664.071989	17.809523
36.254187	1655.667640	17.814541
36.627734	1658.070055	17.819559
36.420079	1662.205332	17.824576
36.778626	1647.467257	17.829594
36.485280	1656.247051	17.834611
36.378066	1645.666826	17.839629
36.698680	1654.913067	17.844647
36.527281	1662.004555	17.849664
36.731844	1664.483378	17.854682
36.530615	1675.466443	17.859699
36.349400	1694.560815	17.864717
36.813499	1682.721388	17.869735
36.815042	1688.045659	17.874752
36.830832	1684.542325	17.879770
36.928982	1677.772976	17.884787
36.904233	1680.672059	17.889805
37.259026	1675.609435	17.894823
36.862794	1688.134649	17.899840
37.125731	1672.180880	17.904858
37.144373	1681.738164	17.909875
37.252029	1698.840603	17.914893
37.531200	1695.129480	17.919911
37.077036	1692.725230	17.924928
37.254869	1694.719899	17.929946
37.505819	1698.204438	17.934963
37.453000	1709.027517	17.939981
37.737296	1714.454978	17.944999
37.572412	1704.018910	17.950016
37.627813	1690.894388	17.955034
37.427921	1683.265328	17.960051
37.480432	1692.539844	17.965069
37.720157	1702.666048	17.970087
37.782277	1707.268873	17.975104
37.818856	1707.192824	17.980122
38.048519	1711.991531	17.985139
37.648278	1696.778658	17.990157
37.740131	1696.840308	17.995175
37.750800	1706.039477	18.000192
37.939519	1707.967777	18.005210
38.110638	1706.580859	18.010227
37.528697	1706.880461	18.015245
38.213266	1701.805348	18.020263
38.155814	1702.265740	18.025280
37.949364	1707.282330	18.030298
38.221955	1697.754541	18.035315
37.865485	1700.743990	18.040333
38.520195	1705.029001	18.045351
38.149541	1708.139699	18.050368
38.353138	1703.792658	18.055386
38.336196	1703.953821	18.060403
38.077767	1699.853761	18.065421
38.328905	1699.546514	18.070439
38.041160	1695.210757	18.075456
38.141143	1693.639161	18.080474
37.960222	1700.803111	18.085491
38.070461	1714.949215	18.090509
38.563680	1735.065825	18.095527
38.307782	1733.988592	18.100544
38.537259	1728.067168	18.105562
38.802600	1728.886317	18.110579
38.513663	1729.864573	18.115597
38.928223	1727.068827	18.120615
38.804589	1728.287822	18.125632
38.889969	1720.933162	18.130650
39.003916	1724.039997	18.135667
39.171719	1732.942687	18.140685
39.137462	1721.541268	18.145703
39.318260	1725.904366	18.150720
39.151043	1725.538046	18.155738
39.119351	1726.198505	18.160755
39.104893	1725.148223	18.165773
39.308673	1724.671256	18.170791
39.199060	1722.667825	18.175808
39.198458	1725.501894	18.180826
39.176560	1718.818548	18.185843
39.219066	1718.055292	18.190861
39.363950	1720.376682	18.195879
39.257017	1720.055105	18.200896
39.429370	1716.639619	18.205914
39.327109	1722.954327	18.210931
39.162170	1723.283304	18.215949
39.825603	1723.928266	18.220967
39.683546	1735.677171	18.225984
39.422303	1715.583741	18.231002
39.904830	1721.287831	18.236019
39.425524	1727.146466	18.241037
39.788803	1734.430949	18.246055
39.704679	1739.896984	18.251072
39.860806	1740.974772	18.256090
39.981500	1742.471424	18.261107
39.702583	1744.531102	18.266125
40.131430	1733.011257	18.271143
40.195240	1737.127586	18.276160
39.966459	1731.960001	18.281178
40.048767	1727.506659	18.286195
40.057614	1743.931803	18.291213
40.297025	1730.458664	18.296231
39.855810	1739.043303	18.301248
40.026323	1736.983248	18.306266
40.545052	1739.350219	18.311283
40.345261	1733.475464	18.316301
40.393543	1738.155787	18.321319
40.270358	1733.271112	18.326336
40.318351	1728.021870	18.331354
40.705432	1732.578373	18.336371
40.379331	1734.680509	18.341389
40.547530	1740.114211	18.346407
40.500607	1732.433812	18.351424
40.572659	1729.964862	18.356442
40.566442	1728.865970	18.361459
40.744178	1727.503545	18.366477
40.857808	1724.235972	18.371495
40.825098	1731.860831	18.376512
40.638762	1727.448823	18.381530
40.692565	1727.430947	18.386547
40.592545	1733.219299	18.391565
40.868484	1726.916556	18.396583
40.592350	1730.658856	18.401600
40.805389	1737.686720	18.406618
40.869132	1725.001343	18.411635
40.634096	1746.850777	18.416653
40.814333	1750.312391	18.421671
40.863569	1758.810317	18.426688
40.869964	1771.455149	18.431706
41.054727	1766.145451	18.436723
40.830195	1762.989772	18.441741
40.946565	1769.764364	18.446759
41.122745	1779.373182	18.451776
41.244830	1788.810646	18.456794
41.312919	1785.966355	18.461811
41.269528	1795.261537	18.466829
41.608380	1787.733376	18.471847
41.421048	1783.553410	18.476864
41.718217	1792.930782	18.481882
41.518923	1781.517276	18.486899
41.685076	1799.940078	18.491917
41.681302	1787.645362	18.496935
41.856808	1779.934801	18.501952
41.944660	1784.626697	18.506970
41.706673	1782.558293	18.511987
41.612648	1790.265381	18.517005
41.809892	1783.270914	18.522023
42.062044	1790.206104	18.527040
42.165579	1797.131654	18.532058
42.129176	1796.953909	18.537075
42.179141	1791.908259	18.542093
41.852752	1783.118585	18.547111
42.401981	1794.144398	18.552128
42.436040	1812.081207	18.557146
42.596244	1797.893557	18.562163
42.470025	1784.685248	18.567181
42.335759	1773.941697	18.572199
42.424060	1777.155152	18.577216
42.534137	1783.578033	18.582234
42.771309	1774.776936	18.587251
42.425368	1776.472121	18.592269
42.159747	1773.213400	18.597287
42.078482	1776.897064	18.602304
42.340499	1782.282568	18.607322
42.637072	1792.884857	18.612339
42.679401	1803.237123	18.617357
42.678951	1807.434191	18.622375
42.761585	1807.752490	18.627392
42.572606	1810.053193	18.632410
42.684448	1796.257416	18.637427
42.559691	1807.947211	18.642445
42.976250	1804.049925	18.647463
42.660077	1808.805185	18.652480
42.732786	1811.401930	18.657498
43.162561	1820.654605	18.662515
43.016484	1828.284503	18.667533
42.895611	1830.898345	18.672551
43.238030	1834.077214	18.677568
43.173620	1833.592684	18.682586
43.483490	1829.792587	18.687603
43.357625	1828.963898	18.692621
43.424953	1831.741461	18.697639
43.399686	1817.721515	18.702656
43.327781	1833.377831	18.707674
43.597977	1814.572277	18.712691
43.461634	1830.896750	18.717709
43.615081	1829.022583	18.722727
43.632532	1825.076023	18.727744
43.804320	1829.222529	18.732762
43.794672	1818.968949	18.737779
43.645443	1821.165825	18.742797
43.518850	1820.962463	18.747815
43.695469	1822.254977	18.752832
43.654561	1829.700924	18.757850
43.889842	1834.772759	18.762867
43.800144	1847.404824	18.767885
44.015435	1852.939825	18.772903
44.218988	1855.050730	18.777920
43.883099	1850.122104	18.782938
44.266005	1841.081481	18.787955
44.088249	1846.789438	18.792973
44.412612	1847.187004	18.797991
44.080067	1845.487011	18.803008
44.193140	1862.681256	18.808026
44.219605	1840.930546	18.813043
44.237986	1841.955165	18.818061
44.152484	1851.897916	18.823079
44.467808	1846.854371	18.828096
44.603391	1865.348849	18.833114
45.143756	1871.956032	18.838131
44.737344	1857.455058	18.843149
44.456058	1847.303133	18.848167
44.890845	1852.795488	18.853184
44.996095	1858.240837	18.858202
45.059042	1846.764173	18.863219
44.801516	1841.599342	18.868237
44.689763	1847.138888	18.873255
45.158919	1856.537821	18.878272
44.901188	1869.227257	18.883290
44.901720	1873.691901	18.888307
45.092169	1871.734829	18.893325
45.243468	1867.374356	18.898343
45.330256	1871.129036	18.903360
45.472027	1867.969374	18.908378
45.086634	1865.159212	18.913395
45.330739	1870.898901	18.918413
45.041490	1864.517640	18.923431
45.512358	1867.655955	18.928448
45.117603	1867.708023	18.933466
45.315999	1862.162567	18.938483
45.457424	1863.673909	18.943501
45.583665	1861.396755	18.948519
45.604720	1862.676056	18.953536
45.363796	1867.282651	18.958554
45.619109	1861.463986	18.963571
45.296341	1855.470176	18.968589
45.159388	1860.755233	18.973607
45.599113	1880.300567	18.978624
45.195468	1897.648523	18.983642
45.289354	1898.622847	18.988659
45.562258	1893.580800	18.993677
45.745803	1913.728449	18.998695
46.292824	1917.911666	19.003712
45.952367	1919.420127	19.008730
46.657438	1923.203939	19.013747
46.910165	1915.244694	19.018765
46.652998	1902.196554	19.023783
46.814179	1886.853914	19.028800
46.808318	1886.491580	19.033818
46.825137	1880.791535	19.038835
46.765381	1878.517619	19.043853
46.652896	1879.423356	19.048871
46.616970	1874.534818	19.053888
46.736221	1881.892850	19.058906
46.900569	1881.528711	19.063923
46.900861	1862.114631	19.068941
46.809917	1861.481736	19.073959
46.652231	1847.462035	19.078976
46.558439	1857.045132	19.083994
46.520210	1876.379441	19.089011
46.767680	1880.214211	19.094029
46.410319	1881.496330	19.099047
46.216762	1880.042615	19.104064
46.445697	1881.974121	19.109082
46.637064	1902.871262	19.114099
47.007552	1902.607636	19.119117
46.982212	1909.908914	19.124135
47.194292	1907.715967	19.129152
46.959570	1907.548225	19.134170
47.378272	1908.554594	19.139187
47.110140	1911.639299	19.144205
46.982271	1906.986845	19.149223
47.214878	1921.538081	19.154240
47.256862	1937.678017	19.159258
47.182209	1937.878659	19.164275
47.287258	1937.411343	19.169293
47.810475	1940.986290	19.174311
47.651749	1928.859250	19.179328
47.595481	1940.916158	19.184346
47.446122	1939.318896	19.189363
47.884036	1932.748693	19.194381
47.621772	1943.209364	19.199399
48.081911	1942.837977	19.204416
47.941006	1957.137309	19.209434
48.019282	1954.651544	19.214451
48.249693	1957.063141	19.219469
48.015424	1960.193825	19.224487
48.222635	1965.699101	19.229504
48.410070	1952.206030	19.234522
48.266626	1944.994275	19.239539
48.175856	1962.278290	19.244557
48.257258	1958.406148	19.249575
48.373974	1947.279177	19.254592
48.305487	1952.651356	19.259610
48.466637	1943.257621	19.264627
48.949367	1939.443048	19.269645
48.342842	1951.098943	19.274663
48.977342	1942.844966	19.279680
48.836209	1954.777352	19.284698
48.897763	1953.386901	19.289715
48.957716	1950.753774	19.294733
48.527595	1950.311293	19.299751
48.549348	1942.877692	19.304768
48.901248	1943.990402	19.309786
48.710953	1943.648764	19.314803
48.981181	1940.598134	19.319821
48.900452	1935.649671	19.324839
48.995786	1938.898611	19.329856
48.459170	1938.887946	19.334874
48.755618	1943.157545	19.339891
49.115406	1962.303218	19.344909
48.996699	1973.270859	19.349927
49.249748	1968.497437	19.354944
49.236651	1982.766180	19.359962
49.152477	1973.629196	19.364979
49.259525	1974.280866	19.369997
49.080330	1978.332770	19.375015
49.364500	1984.300912	19.380032
49.545549	1995.158695	19.385050
49.797112	2005.875673	19.390067
49.798210	2001.827049	19.395085
49.616343	2005.780582	19.400103
50.073759	2001.726872	19.405120
49.932849	1995.139099	19.410138
49.863772	2002.998465	19.415155
50.119082	1986.827127	19.420173
49.970830	2002.686418	19.425191
49.836629	1999.331475	19.430208
49.920779	1998.154607	19.435226
49.941167	1995.022499	19.440243
50.511094	1990.676139	19.445261
50.239615	1995.953990	19.450279
50.178039	1989.736557	19.455296
50.381180	1984.346969	19.460314
50.665358	1990.944262	19.465331
50.650388	1987.636509	19.470349
50.289511	1986.420337	19.475367
50.666281	1986.059605	19.480384
50.404740	1983.298207	19.485402
50.531273	2002.115614	19.490419
50.750781	2003.667191	19.495437
50.597377	2021.590793	19.500455
50.843439	2012.893605	19.505472
51.077885	2017.490823	19.510490
50.906877	2019.661805	19.515507
51.298700	2009.893210	19.520525
51.076881	2010.900527	19.525543
51.250252	2013.138502	19.530560
51.206960	2014.145785	19.535578
50.707068	2015.261747	19.540595
51.304771	2013.013200	19.545613
51.090665	2014.614531	19.550631
51.397870	2019.498528	19.555648
51.317740	2004.550858	19.560666
51.219839	2009.351534	19.565683
51.405246	2008.982723	19.570701
51.405495	2008.613075	19.575719
51.503372	2004.820873	19.580736
51.199036	2009.481318	19.585754
51.214710	2024.655596	19.590771
51.358538	2030.985980	19.595789
51.190937	2031.982351	19.600807
51.239231	2036.010382	19.605824
51.680008	2035.644562	19.610842
51.761025	2057.717696	19.615859
52.079493	2062.763233	19.620877
51.958956	2060.552112	19.625895
51.956831	2062.821910	19.630912
52.198002	2053.085321	19.635930
52.296039	2064.522270	19.640947
52.408120	2058.826071	19.645965
52.340826	2063.345310	19.650983
52.543725	2060.879445	19.656000
52.717886	2063.676763	19.661018
52.423561	2062.894066	19.666035
52.865417	2054.517988	19.671053
52.764503	2050.803575	19.676071
52.784197	2052.073273	19.681088
52.892739	2056.685445	19.686106
52.708122	2045.820511	19.691123
52.960956	2041.380182	19.696141
52.687134	2050.522329	19.701159
52.833757	2044.803880	19.706176
53.136020	2050.163129	19.711194
52.684638	2058.951993	19.716211
52.884160	2055.541779	19.721229
53.048967	2054.968892	19.726247
53.010879	2054.311488	19.731264
53.323266	2042.576835	19.736282
52.787890	2054.543475	19.741299
53.228847	2050.560590	19.746317
53.006573	2046.670599	19.751335
53.288929	2050.134270	19.756352
53.367368	2036.719019	19.761370
53.109640	2046.514422	19.766387
53.411485	2061.120075	19.771405
53.636107	2072.313621	19.776423
53.526955	2077.252800	19.781440
53.933877	2067.424975	19.786458
53.593682	2078.880560	19.791475
53.667667	2075.245058	19.796493
53.902249	2069.114779	19.801511
53.593371	2073.473623	19.806528
53.903167	2064.867824	19.811546
53.879939	2073.434616	19.816563
54.111617	2069.632448	19.821581
54.317775	2066.058529	19.826599
54.332740	2086.295342	19.831616
54.284311	2070.364375	19.836634
53.998591	2072.170095	19.841651
54.327731	2088.324845	19.846669
54.396923	2100.884348	19.851687
54.391234	2100.898371	19.856704
54.639671	2102.327448	19.861722
54.482417	2105.025708	19.866739
55.053589	2098.497153	19.871757
54.831085	2101.492054	19.876775
54.739123	2105.106698	19.881792
54.863862	2093.950340	19.886810
54.895351	2103.665605	19.891827
55.128734	2098.717835	19.896845
55.176938	2099.854072	19.901863
54.972403	2104.490539	19.906880
55.207699	2103.183121	19.911898
54.987100	2095.155698	19.916915
54.893656	2103.089623	19.921933
54.935041	2097.969308	19.926951
54.763917	2091.060896	19.931968
55.007578	2095.739292	19.936986
54.887934	2100.624701	19.942003
55.266735	2108.367831	19.947021
55.417523	2116.598735	19.952039
55.127686	2125.277419	19.957056
55.450004	2126.094245	19.962074
55.263358	2120.851832	19.967091
55.323075	2124.480737	19.972109
55.110751	2123.214364	19.977127
55.048193	2138.259970	19.982144
55.771336	2149.808835	19.987162
55.829062	2150.074571	19.992179
55.673554	2149.009819	19.997197
55.867898	2146.752058	20.002215
55.959886	2156.033307	20.007232
56.136298	2147.928700	20.012250
55.804379	2146.519917	20.017267
56.089451	2146.833445	20.022285
56.145046	2173.295360	20.027303
56.201173	2184.119234	20.032320
56.392469	2178.346093	20.037338
56.639347	2171.455049	20.042355
56.873899	2169.841831	20.047373
57.154888	2169.006781	20.052391
56.933366	2172.104685	20.057408
56.710052	2155.427758	20.062426
56.464485	2157.317787	20.067443
56.743429	2164.842826	20.072461
57.132303	2159.562192	20.077479
57.139314	2167.768503	20.082496
57.366196	2159.275992	20.087514
57.236096	2168.040460	20.092531
57.128849	2158.606389	20.097549
57.155128	2143.518125	20.102567
56.983203	2161.106361	20.107584
57.158535	2165.325602	20.112602
57.002355	2169.584776	20.117619
57.144470	2166.556105	20.122637
57.213064	2160.084758	20.127655
57.072177	2160.629847	20.132672
57.429033	2157.449867	20.137690
57.234724	2170.194008	20.142707
57.461338	2189.541941	20.147725
57.790824	2195.136505	20.152743
57.525038	2190.654053	20.157760
57.207471	2193.812748	20.162778
57.652927	2196.428549	20.167795
57.673675	2203.598313	20.172813
57.577715	2199.231837	20.177831
58.033400	2213.464904	20.182848
58.005325	2224.907891	20.187866
57.757246	2229.164975	20.192883
58.023241	2229.677734	20.197901
58.425607	2220.547840	20.202919
57.791117	2223.803509	20.207936
58.242850	2219.941638	20.212954
58.477514	2231.560819	20.217971
58.576444	2239.736593	20.222989
58.895480	2247.449923	20.228007
58.990412	2245.574372	20.233024
58.908388	2222.644980	20.238042
58.794752	2214.913970	20.243059
58.543732	2220.913340	20.248077
58.942931	2227.907059	20.253095
58.850317	2241.758087	20.258112
59.151766	2235.287524	20.263130
58.998912	2242.796694	20.268147
59.120590	2242.025816	20.273165
59.561947	2249.265725	20.278183
59.121138	2246.952483	20.283200
59.277862	2240.453124	20.288218
59.468208	2242.344608	20.293235
59.120976	2248.018173	20.298253
59.620410	2235.846481	20.303271
59.518525	2244.603563	20.308288
59.525369	2242.376048	20.313306
59.281850	2244.185035	20.318323
59.254009	2241.716403	20.323341
59.500650	2239.497215	20.328359
59.342658	2245.859552	20.333376
59.704884	2237.261908	20.338394
59.824501	2250.939213	20.343411
59.979446	2264.999674	20.348429
60.668219	2255.925096	20.353447
60.174243	2245.961676	20.358464
59.966253	2233.972874	20.363482
60.427298	2227.333755	20.368499
60.063047	2249.380100	20.373517
60.579585	2253.564522	20.378535
60.290417	2259.940711	20.383552
60.665651	2253.966606	20.388570
60.891637	2253.538707	20.393587
60.349560	2255.844789	20.398605
60.699546	2245.857769	20.403623
60.857912	2254.895399	20.408640
60.760616	2248.085721	20.413658
61.055604	2242.159161	20.418675
61.136212	2255.448425	20.423693
61.251918	2239.484989	20.428711
61.137908	2244.281318	20.433728
61.014434	2231.676530	20.438746
61.182506	2236.376540	20.443763
61.093100	2236.272529	20.448781
61.369527	2234.065734	20.453799
61.201345	2241.349479	20.458816
60.906038	2248.571991	20.463834
60.755141	2235.888666	20.468851
60.945764	2242.626366	20.473869
61.251752	2245.712532	20.478887
61.427116	2262.491771	20.483904
61.631101	2265.255446	20.488922
61.539336	2270.161096	20.493939
61.540428	2275.053341	20.498957
61.626135	2272.004066	20.503975
61.695290	2277.925638	20.508992
61.764619	2284.698402	20.514010
62.054304	2276.601352	20.519027
61.845671	2274.833545	20.524045
61.762071	2279.809503	20.529063
61.706907	2296.567105	20.534080
61.732394	2290.336711	20.539098
61.940660	2297.459719	20.544115
61.921504	2311.976629	20.549133
62.243446	2319.763140	20.554151
62.266305	2332.348220	20.559168
62.584249	2327.691115	20.564186
62.511720	2328.811139	20.569203
62.570335	2331.402037	20.574221
62.729087	2328.534760	20.579239
62.385637	2325.914820	20.584256
62.588304	2342.958141	20.589274
62.688294	2350.648736	20.594291
62.779079	2350.114081	20.599309
63.263351	2354.232217	20.604327
62.896990	2358.412066	20.609344
62.912485	2357.432769	20.614362
63.401912	2356.134040	20.619379
63.290338	2359.948064	20.624397
63.471993	2348.855725	20.629415
63.038783	2346.817995	20.634432
63.452847	2341.833537	20.639450
63.793006	2348.818190	20.644467
63.649092	2348.837383	20.649485
63.635857	2344.972941	20.654503
63.555790	2350.176694	20.659520
63.571785	2358.327285	20.664538
63.872493	2366.390577	20.669555
64.001833	2373.795207	20.674573
64.017064	2363.644633	20.679591
64.144637	2375.321027	20.684608
63.728304	2370.677219	20.689626
64.071788	2369.914886	20.694643
63.728663	2372.540814	20.699661
64.031593	2368.145645	20.704679
63.894917	2378.571638	20.709696
64.254944	2396.129539	20.714714
64.587242	2396.526202	20.719731
64.426324	2392.638956	20.724749
64.587131	2387.935408	20.729767
64.602615	2397.499955	20.734784
64.549649	2398.326178	20.739802
64.909410	2386.462157	20.744819
64.653455	2397.692598	20.749837
64.842568	2390.774800	20.754855
65.020083	2409.564180	20.759872
65.098213	2420.231812	20.764890
65.427194	2411.938805	20.769907
65.280339	2422.633062	20.774925
65.552796	2413.212346	20.779943
65.437484	2419.659030	20.784960
65.480346	2425.383427	20.789978
65.977046	2414.830639	20.794995
66.032383	2417.764238	20.800013
65.589149	2387.997988	20.805031
65.776724	2374.000567	20.810048
65.692102	2380.522079	20.815066
65.778498	2387.118825	20.820083
65.730994	2410.612631	20.825101
65.982810	2392.910663	20.830119
66.166805	2401.087792	20.835136
65.716136	2407.466766	20.840154
66.154443	2398.618628	20.845171
66.188776	2407.059137	20.850189
66.095992	2401.701475	20.855207
66.089626	2406.568223	20.860224
66.215408	2413.782901	20.865242
66.448355	2406.329464	20.870259
66.123134	2410.372586	20.875277
66.287656	2423.967408	20.880295
66.249318	2426.076318	20.885312
66.129573	2439.557190	20.890330
66.432230	2426.810814	20.895347
66.735737	2452.173830	20.900365
66.976977	2457.037392	20.905383
66.735454	2467.133148	20.910400
67.050329	2470.806897	20.915418
67.128815	2460.040241	20.920435
67.459242	2468.385296	20.925453
67.254122	2466.069217	20.930471
67.481052	2459.759334	20.935488
67.232975	2460.800948	20.940506
67.606089	2457.903272	20.945523
67.228912	2462.347158	20.950541
67.061720	2462.221378	20.955559
67.314126	2467.553987	20.960576
67.686835	2482.177045	20.965594
68.082985	2482.179652	20.970611
67.590765	2488.662395	20.975629
67.952457	2480.900974	20.980647
67.802790	2491.066185	20.985664
67.790867	2492.231700	20.990682
68.263293	2480.184771	20.995699
67.982536	2485.760007	21.000717
67.893068	2492.922169	21.005735
68.304945	2481.858548	21.010752
68.146250	2487.360028	21.015770
68.122088	2483.939906	21.020787
68.131747	2507.115713	21.025805
68.488109	2505.676005	21.030823
68.487361	2500.436149	21.035840
68.596071	2510.392833	21.040858
68.974846	2501.632058	21.045875
68.803489	2503.667723	21.050893
69.079819	2498.435929	21.055911
68.971387	2508.969543	21.060928
69.098540	2496.564787	21.065946
69.048670	2495.249828	21.070963
69.207064	2500.270830	21.075981
69.053902	2503.448037	21.080999
68.939720	2503.870992	21.086016
69.281810	2523.261248	21.091034
69.659877	2521.159244	21.096051
69.571201	2526.960185	21.101069
69.561010	2529.648342	21.106087
69.741959	2525.219780	21.111104
69.678524	2522.286496	21.116122
69.938122	2520.875409	21.121139
69.783330	2527.319225	21.126157
69.982371	2524.349173	21.131175
69.906090	2518.547374	21.136192
69.889722	2520.385714	21.141210
70.192319	2512.843917	21.146227
70.220507	2534.424084	21.151245
70.509388	2553.566480	21.156263
70.170203	2547.810564	21.161280
70.367333	2557.627040	21.166298
70.487879	2549.171611	21.171315
70.874186	2547.509999	21.176333
70.170385	2560.484892	21.181351
70.416017	2545.942238	21.186368
70.537629	2556.290147	21.191386
70.606692	2545.288363	21.196403
70.653267	2561.977826	21.201421
70.776150	2574.388656	21.206439
70.986047	2580.492957	21.211456
71.009790	2578.501587	21.216474
71.426341	2577.275937	21.221491
71.458421	2573.339758	21.226509
71.427439	2575.147845	21.231527
71.493024	2564.313170	21.236544
71.231422	2576.267553	21.241562
71.367853	2578.040833	21.246579
71.514364	2572.037940	21.251597
71.943772	2590.253907	21.256615
71.829716	2602.127577	21.261632
71.957985	2600.476400	21.266650
72.157423	2596.590461	21.271667
72.121859	2601.831420	21.276685
72.115197	2595.025088	21.281703
72.350695	2600.944832	21.286720
72.610484	2595.580696	21.291738
72.505599	2597.227389	21.296755
72.802006	2587.267529	21.301773
72.535649	2575.798002	21.306791
72.365537	2563.818815	21.311808
72.292529	2572.038196	21.316826
72.562425	2581.828464	21.321843
72.594025	2586.754734	21.326861
72.426616	2588.704711	21.331879
72.897594	2585.252585	21.336896
72.538989	2599.024343	21.341914
72.565296	2587.565012	21.346931
72.463733	2590.717943	21.351949
72.897602	2613.981553	21.356967
73.108591	2615.883840	21.361984
72.873680	2625.677008	21.367002
73.139448	2622.422642	21.372019
73.011697	2623.302208	21.377037
72.999107	2629.305564	21.382055
73.206373	2632.382168	21.387072
73.145302	2652.184640	21.392090
73.168842	2657.998547	21.397107
73.771517	2653.281996	21.402125
73.544384	2658.307432	21.407143
73.952880	2664.988373	21.412160
73.927082	2672.500335	21.417178
74.395945	2668.589848	21.422195
74.755684	2668.752433	21.427213
74.604287	2672.757391	21.432231
74.755629	2648.753225	21.437248
74.403263	2647.163122	21.442266
74.157032	2634.864966	21.447283
74.874229	2636.407041	21.452301
74.691349	2655.732802	21.457319
75.124631	2652.458962	21.462336
74.807361	2647.460455	21.467354
75.032751	2648.441796	21.472371
75.033897	2635.707376	21.477389
74.924154	2646.466118	21.482407
75.236179	2637.573791	21.487424
75.263543	2654.821296	21.492442
75.313475	2653.029137	21.497459
74.934266	2651.593094	21.502477
74.656999	2655.372022	21.507495
75.288860	2646.640132	21.512512
75.034839	2653.799297	21.517530
75.501389	2667.116354	21.522547
75.809219	2680.692790	21.527565
75.500910	2684.925715	21.532583
75.795361	2679.531794	21.537600
75.729206	2686.617738	21.542618
75.629211	2684.362177	21.547635
75.837513	2676.940254	21.552653
75.639452	2683.694863	21.557671
75.909302	2696.912616	21.562688
75.862868	2710.327643	21.567706
75.988376	2702.496158	21.572723
76.211237	2704.282309	21.577741
76.128756	2712.975019	21.582759
76.372220	2712.096545	21.587776
76.291214	2726.370914	21.592794
76.458521	2743.419349	21.597811
76.620162	2733.641959	21.602829
76.827620	2745.526679	21.607847
76.947808	2739.216247	21.612864
76.909592	2736.829574	21.617882
76.713972	2738.128287	21.622899
77.032878	2745.613920	21.627917
77.027758	2754.495433	21.632935
77.021791	2751.579757	21.637952
77.502050	2760.883699	21.642970
77.138510	2758.829257	21.647987
77.695997	2752.413339	21.653005
77.590672	2754.562127	21.658023
78.062309	2744.709383	21.663040
77.975541	2742.986703	21.668058
77.909097	2744.926281	21.673075
78.082654	2734.643337	21.678093
77.671644	2748.679433	21.683111
78.196730	2750.842351	21.688128
78.427105	2745.075918	21.693146
78.092986	2747.731127	21.698163
78.333116	2738.828992	21.703181
78.141409	2745.201839	21.708199
78.522857	2754.119746	21.713216
78.711132	2763.010584	21.718234
78.698664	2774.730940	21.723251
78.660145	2770.091386	21.728269
78.563533	2767.331672	21.733287
78.541579	2763.117363	21.738304
78.644195	2773.542582	21.743322
78.966797	2769.690937	21.748339
78.744787	2756.414979	21.753357
78.984895	2770.838203	21.758375
78.925595	2788.910896	21.763392
79.199430	2788.761304	21.768410
79.407991	2797.225149	21.773427
79.515296	2793.848550	21.778445
79.628788	2802.311601	21.783463
79.531620	2792.419535	21.788480
79.842839	2793.852852	21.793498
79.517165	2792.162242	21.798515
79.709523	2783.702277	21.803533
79.697439	2796.754971	21.808551
80.301355	2812.206661	21.813568
80.263159	2817.445372	21.818586
80.206147	2827.426155	21.823603
80.412717	2828.061778	21.828621
80.565433	2821.921137	21.833639
80.367199	2814.730648	21.838656
80.581234	2820.009098	21.843674
80.304277	2821.231121	21.848691
80.576613	2812.188955	21.853709
80.843907	2813.819719	21.858727
80.735107	2811.021067	21.863744
80.393036	2812.477904	21.868762
80.727409	2829.240088	21.873779
80.826238	2833.759998	21.878797
80.814630	2846.091336	21.883815
81.018518	2846.166335	21.888832
80.945511	2842.415218	21.893850
81.069447	2850.371015	21.898867
81.327797	2866.828873	21.903885
81.346493	2873.922113	21.908903
81.646358	2864.487927	21.913920
81.704797	2865.442590	21.918938
81.853272	2866.208709	21.923955
82.090598	2863.636618	21.928973
81.810360	2856.585682	21.933991
81.698874	2865.512826	21.939008
81.818007	2887.286314	21.944026
82.029329	2899.069716	21.949043
82.495510	2884.741826	21.954061
82.391145	2897.554744	21.959079
82.458135	2892.731529	21.964096
82.663444	2893.526431	21.969114
82.443480	2897.084099	21.974131
82.853720	2897.646234	21.979149
82.623642	2895.629916	21.984167
82.617439	2894.827027	21.989184
82.980215	2906.846404	21.994202
82.723047	2920.671339	21.999219
82.912890	2924.321802	22.004237
83.051896	2922.846782	22.009255
83.239934	2920.619091	22.014272
83.400931	2917.249325	22.019290
83.171794	2923.856414	22.024307
83.574441	2921.248672	22.029325
83.275828	2922.254978	22.034343
83.430026	2915.786862	22.039360
83.648015	2926.725016	22.044378
83.824903	2945.221027	22.049395
84.279551	2942.630264	22.054413
83.838854	2947.706904	22.059431
84.036444	2942.653369	22.064448
84.152784	2946.169145	22.069466
83.798867	2946.102626	22.074483
84.103028	2946.596493	22.079501
84.219508	2944.796038	22.084519
84.387425	2963.485305	22.089536
84.591690	2969.216251	22.094554
84.485449	2969.874144	22.099571
84.996595	2970.377838	22.104589
84.514572	2967.877984	22.109607
84.904179	2972.270647	22.114624
84.945667	2970.036110	22.119642
84.748563	2968.623825	22.124659
84.914635	2963.629444	22.129677
85.382122	2997.264171	22.134695
85.149388	3000.861776	22.139712
85.667428	2993.795934	22.144730
85.416035	2996.152422	22.149747
85.818800	2994.013194	22.154765
85.622636	2991.174639	22.159783
85.527869	2995.823904	22.164800
86.035116	2986.606510	22.169818
85.757491	2995.368700	22.174835
85.687853	2986.669304	22.179853
86.062716	3009.577496	22.184871
85.869392	3022.695430	22.189888
85.879163	3022.096208	22.194906
85.945701	3031.358963	22.199923
86.371403	3023.662275	22.204941
86.247487	3027.011532	22.209959
86.653365	3036.269289	22.214976
86.610248	3045.771489	22.219994
86.694370	3046.897912	22.225011
86.783218	3041.822189	22.230029
87.038424	3032.429158	22.235047
86.890386	3033.720409	22.240064
87.306670	3024.662950	22.245082
87.133843	3043.891848	22.250099
87.369503	3062.838547	22.255117
87.682718	3063.024591	22.260135
87.717868	3061.779767	22.265152
87.714873	3057.710284	22.270170
87.746197	3061.624450	22.275187
87.793652	3067.419195	22.280205
87.894142	3067.515647	22.285223
87.805887	3064.211138	22.290240
87.911029	3065.554181	22.295258
87.838987	3068.631053	22.300275
87.905375	3064.564649	22.305293
88.174948	3074.722246	22.310311
88.054466	3088.022680	22.315328
88.645735	3089.500215	22.320346
88.385515	3093.739855	22.325363
88.333032	3090.153012	22.330381
88.546485	3093.935446	22.335399
88.404056	3090.554854	22.340416
88.726109	3105.270755	22.345434
88.734757	3117.698964	22.350451
88.952882	3110.094877	22.355469
88.888876	3112.002991	22.360487
88.700048	3122.771217	22.365504
89.138542	3111.814569	22.370522
89.087324	3122.423383	22.375539
89.145189	3134.301277	22.380557
89.504092	3138.969571	22.385575
89.444901	3145.387181	22.390592
89.748012	3141.744599	22.395610
89.563965	3136.653788	22.400627
89.826333	3135.238645	22.405645
90.165163	3154.051038	22.410663
89.969908	3162.112212	22.415680
90.421559	3167.916848	22.420698
90.212401	3171.516888	22.425715
90.356473	3164.927499	22.430733
90.587155	3154.413145	22.435751
90.867692	3176.362695	22.440768
90.897500	3152.264482	22.445786
90.596428	3161.601963	22.450803
91.064486	3158.343525	22.455821
90.958965	3155.511981	22.460839
90.481192	3167.922334	22.465856
91.030732	3164.840580	22.470874
91.393134	3178.092242	22.475891
91.269858	3181.263849	22.480909
91.612815	3175.003373	22.485927
91.619588	3180.381625	22.490944
91.537048	3180.539095	22.495962
91.638397	3173.116140	22.500979
91.966415	3177.845865	22.505997
91.791187	3175.978317	22.511015
91.632706	3186.387196	22.516032
91.724734	3183.355992	22.521050
92.116288	3194.714854	22.526067
92.008945	3205.811019	22.531085
92.464805	3208.118157	22.536103
92.553939	3204.685024	22.541120
92.628138	3205.057905	22.546138
92.824062	3197.120016	22.551155
92.496421	3209.539012	22.556173
92.977247	3202.735565	22.561191
92.546269	3205.016295	22.566208
92.763470	3206.478606	22.571226
93.143731	3213.255809	22.576243
92.953724	3224.846433	22.581261
93.122767	3234.824697	22.586279
93.089413	3230.329442	22.591296
93.036485	3227.734872	22.596314
93.306628	3227.311845	22.601331
93.159038	3225.522795	22.606349
93.595046	3239.248200	22.611367
93.688040	3258.365230	22.616384
94.026196	3253.803337	22.621402
93.677032	3265.647139	22.626419
93.892952	3255.970291	22.631437
94.161553	3260.596875	22.636455
94.387719	3267.780366	22.641472
94.376497	3271.709111	22.646490
94.390855	3284.102645	22.651507
94.646546	3276.863163	22.656525
94.734561	3286.455227	22.661543
94.559994	3277.519865	22.666560
94.925247	3275.456899	22.671578
94.851539	3277.863149	22.676595
94.562205	3283.125486	22.681613
95.288305	3269.236939	22.686631
95.269679	3278.320221	22.691648
95.370369	3275.249371	22.696666
95.317090	3280.684062	22.701683
95.256510	3296.062382	22.706701
95.705433	3297.087472	22.711719
95.187715	3308.740687	22.716736
95.597736	3304.575587	22.721754
95.309833	3301.447406	22.726771
95.354270	3297.939361	22.731789
95.276939	3311.737620	22.736807
95.740859	3326.413310	22.741824
96.017167	3328.300933	22.746842
96.002266	3324.562916	22.751859
96.090376	3348.210108	22.756877
96.670065	3353.717993	22.761895
96.591755	3359.425784	22.766912
96.719015	3361.565675	22.771930
96.853151	3353.606438	22.776947
96.686101	3357.208997	22.781965
96.916676	3350.539452	22.786983
97.090461	3349.988660	22.792000
97.320981	3369.247641	22.797018
97.101648	3380.114806	22.802035
97.513730	3381.609047	22.807053
97.800985	3368.670341	22.812071
97.820692	3377.426430	22.817088
97.918662	3375.925876	22.822106
98.102478	3370.069669	22.827123
98.015638	3369.717952	22.832141
98.095676	3366.032717	22.837159
97.946038	3363.672272	22.842176
98.388157	3361.934401	22.847194
98.251725	3361.420404	22.852211
98.385765	3368.445553	22.857229
98.590413	3361.018399	22.862247
98.586345	3367.031259	22.867264
98.141368	3362.262743	22.872282
98.889384	3393.203153	22.877299
98.423112	3403.469021	22.882317
98.773719	3398.881007	22.887335
98.623141	3405.919830	22.892352
98.716290	3404.067274	22.897370
98.828092	3414.475258	22.902387
99.121615	3413.101395	22.907405
99.192079	3416.265383	22.912423
99.382566	3420.085168	22.917440
99.348046	3430.756788	22.922458
99.749281	3435.612674	22.927475
99.413387	3446.635815	22.932493
99.679719	3446.896960	22.937511
99.673180	3444.367909	22.942528
99.745573	3459.765716	22.947546
100.024369	3463.477966	22.952563
99.920025	3473.691041	22.957581
100.582888	3462.479652	22.962599
100.254432	3477.388268	22.967616
100.395321	3477.068536	22.972634
100.848819	3492.083551	22.977651
100.727160	3504.919516	22.982669
101.056310	3501.898996	22.987687
100.872645	3498.601922	22.992704
100.750795	3498.804885	22.997722
101.400147	3505.677050	23.002739
101.239838	3499.697042	23.007757
101.408958	3508.294985	23.012775
101.384708	3512.658283	23.017792
101.416736	3527.475761	23.022810
101.984428	3526.457724	23.027827
101.897313	3527.955490	23.032845
102.141074	3521.737683	23.037863
101.841225	3517.388057	23.042880
102.084425	3519.200862	23.047898
101.983713	3520.399267	23.052915
101.818972	3521.451954	23.057933
102.160703	3533.035483	23.062951
102.411662	3558.350333	23.067968
102.307693	3551.401014	23.072986
102.528976	3545.420413	23.078003
102.724587	3547.546257	23.083021
102.879090	3548.779189	23.088039
102.664090	3570.779841	23.093056
102.902482	3570.146682	23.098074
103.335046	3575.888877	23.103091
103.128853	3584.864398	23.108109
103.213394	3568.456677	23.113127
103.678395	3580.572263	23.118144
103.367980	3593.662023	23.123162
103.859283	3590.815057	23.128179
103.835653	3595.994129	23.133197
104.214150	3586.178334	23.138215
104.431810	3591.593078	23.143232
104.060573	3595.847295	23.148250
104.343435	3584.794419	23.153267
104.555964	3583.466634	23.158285
104.391019	3579.718749	23.163303
104.407623	3590.784427	23.168320
104.407241	3600.146013	23.173338
104.913688	3611.531439	23.178355
105.140301	3610.402133	23.183373
104.967429	3614.995213	23.188391
105.448148	3610.641927	23.193408
104.723353	3615.802829	23.198426
105.480289	3615.244856	23.203443
105.460016	3625.548455	23.208461
105.680568	3616.214363	23.213479
105.876562	3628.294201	23.218496
105.538394	3640.990513	23.223514
105.682644	3642.924060	23.228531
105.788093	3649.403998	23.233549
105.968782	3638.087650	23.238567
105.813750	3643.568845	23.243584
105.965212	3648.775644	23.248602
106.428628	3665.378763	23.253619
106.367673	3669.993098	23.258637
106.422851	3668.242480	23.263655
106.374572	3665.936082	23.268672
106.186204	3669.915519	23.273690
106.549646	3689.141862	23.278707
106.830261	3692.827091	23.283725
107.297262	3691.556783	23.288743
107.191867	3687.082774	23.293760
107.079410	3698.892829	23.298778
107.423118	3709.889862	23.303795
107.316812	3722.591556	23.308813
107.968446	3719.503425	23.313831
107.874492	3715.403156	23.318848
108.004498	3715.628209	23.323866
108.260750	3711.080140	23.328883
108.247383	3724.958342	23.333901
108.467358	3719.215720	23.338919
108.478829	3713.809632	23.343936
108.466854	3716.006094	23.348954
108.608033	3713.822278	23.353971
108.451849	3713.866732	23.358989
108.940104	3727.625656	23.364007
109.131539	3734.334339	23.369024
108.711245	3749.721080	23.374042
109.351680	3744.942046	23.379059
108.987258	3744.915846	23.384077
109.188727	3743.442221	23.389095
109.045307	3739.462356	23.394112
109.365804	3742.237719	23.399130
109.371106	3739.956302	23.404147
109.377445	3752.057005	23.409165
109.502459	3763.037917	23.414183
109.799824	3769.752701	23.419200
109.544210	3775.897143	23.424218
109.723603	3771.177898	23.429235
109.808341	3800.105807	23.434253
110.030016	3796.258025	23.439271
110.472989	3804.285519	23.444288
110.263783	3810.953074	23.449306
110.194683	3805.569744	23.454323
110.148110	3815.674250	23.459341
110.613065	3830.920011	23.464359
110.940801	3819.700069	23.469376
110.432926	3833.918942	23.474394
110.928078	3842.820226	23.479411
111.171061	3849.927175	23.484429
111.011646	3851.832669	23.489447
111.548454	3856.016148	23.494464
112.010809	3872.016820	23.499482
112.436911	3865.567083	23.504499
112.086496	3877.174509	23.509517
111.984899	3868.856740	23.514535
112.458063	3863.216654	23.519552
112.582253	3871.940758	23.524570
112.590184	3867.907844	23.529587
112.472673	3869.660711	23.534605
112.507272	3869.737366	23.539623
112.876332	3870.101607	23.544640
112.745510	3857.559721	23.549658
112.706848	3861.419918	23.554675
112.727939	3874.782237	23.559693
112.796961	3889.554162	23.564711
113.223703	3888.200729	23.569728
113.144764	3901.074046	23.574746
113.337132	3904.141953	23.579763
113.762384	3901.059376	23.584781
113.680503	3911.688764	23.589799
113.799925	3915.034145	23.594816
113.750456	3927.609648	23.599834
114.210885	3930.263832	23.604851
114.097391	3921.301057	23.609869
114.001915	3914.875838	23.614887
114.484988	3925.502260	23.619904
114.550396	3951.174896	23.624922
114.869946	3946.306390	23.629939
114.727607	3936.693166	23.634957
114.893311	3945.701820	23.639975
115.166357	3942.527883	23.644992
115.102891	3947.113970	23.650010
114.971026	3942.052449	23.655027
115.126483	3939.304343	23.660045
115.190789	3963.136747	23.665063
115.198114	3961.299123	23.670080
115.592887	3968.664896	23.675098
115.619426	3967.072948	23.680115
115.608984	3972.529924	23.685133
115.535465	3985.007864	23.690151
115.964594	3995.364483	23.695168
115.835895	4010.714224	23.700186
116.024294	4001.613217	23.705203
116.191718	4015.676736	23.710221
116.502443	4018.758933	23.715239
116.396397	4024.994867	23.720256
116.437995	4026.115015	23.725274
116.507267	4028.385091	23.730291
116.479280	4024.685299	23.735309
116.624185	4040.959212	23.740327
116.874763	4050.452377	23.745344
116.971601	4048.289637	23.750362
117.458240	4074.747984	23.755379
117.724149	4081.117662	23.760397
117.847978	4079.225297	23.765415
117.893568	4084.510017	23.770432
118.071787	4084.453034	23.775450
118.312735	4086.203277	23.780467
118.274073	4079.053510	23.785485
118.186708	4075.172169	23.790503
118.338304	4070.779536	23.795520
118.500986	4079.266637	23.800538
118.466235	4096.027118	23.805555
119.035411	4101.465350	23.810573
118.712323	4100.208485	23.815591
119.037017	4098.089128	23.820608
118.979822	4102.104839	23.825626
119.229047	4098.496950	23.830643
119.537111	4091.259844	23.835661
119.538435	4118.618435	23.840679
119.800298	4120.115572	23.845696
119.414552	4126.994803	23.850714
119.598717	4122.239225	23.855731
120.217651	4113.084196	23.860749
119.852516	4117.772256	23.865767
120.272644	4122.318490	23.870784
120.381642	4133.327514	23.875802
120.352894	4140.512269	23.880819
120.797457	4140.586806	23.885837
120.528405	4142.975917	23.890855
120.841566	4130.890704	23.895872
120.763784	4140.250858	23.900890
120.911441	4141.829909	23.905907
121.527791	4144.893031	23.910925
121.201020	4162.133498	23.915943
121.305147	4158.984336	23.920960
121.385344	4162.094493	23.925978
121.533204	4165.280864	23.930995
121.748973	4182.371673	23.936013
121.649000	4191.049591	23.941031
121.774988	4187.485712	23.946048
121.855007	4194.058684	23.951066
122.172922	4198.549410	23.956083
122.561347	4190.347615	23.961101
122.451127	4217.421645	23.966119
122.606499	4217.843328	23.971136
122.585696	4230.224531	23.976154
122.750023	4218.834084	23.981171
122.875389	4211.905959	23.986189
122.917584	4228.718419	23.991207
123.182908	4237.424085	23.996224
123.273765	4250.711383	24.001242
123.281458	4248.796487	24.006259
123.219840	4245.471565	24.011277
123.237220	4256.481669	24.016295
123.561506	4263.449734	24.021312
123.497072	4279.549858	24.026330
123.590261	4284.198310	24.031347
124.205461	4298.751822	24.036365
123.979164	4302.568771	24.041383
124.279639	4302.056826	24.046400
124.648755	4291.046665	24.051418
124.490136	4296.033713	24.056435
125.038965	4297.707017	24.061453
125.050385	4322.375637	24.066471
125.291008	4329.100846	24.071488
125.224211	4333.621444	24.076506
125.491395	4324.356786	24.081523
125.725087	4319.883551	24.086541
125.607471	4322.739039	24.091559
125.775693	4315.663591	24.096576
125.905794	4319.596370	24.101594
125.573786	4318.431531	24.106611
126.076754	4310.134317	24.111629
126.030096	4341.104227	24.116647
126.478205	4336.148952	24.121664
126.777185	4345.248388	24.126682
126.668345	4341.665864	24.131699
126.837965	4335.984121	24.136717
127.065004	4344.626095	24.141735
127.153866	4346.101496	24.146752
127.317320	4339.710411	24.151770
126.967137	4349.804100	24.156787
127.439425	4340.128242	24.161805
127.137354	4354.394230	24.166823
127.277430	4370.659047	24.171840
127.579851	4369.121399	24.176858
127.415870	4373.932950	24.181875
127.562681	4384.779169	24.186893
127.654516	4402.653079	24.191911
127.911119	4409.106337	24.196928
128.223716	4411.780357	24.201946
127.952226	4429.969616	24.206963
128.318417	4431.701526	24.211981
128.300620	4442.717585	24.216999
128.498850	4451.451017	24.222016
128.718268	4461.431569	24.227034
128.595693	4465.733839	24.232051
129.081504	4471.797928	24.237069
129.302613	4489.429232	24.242087
129.212566	4490.401887	24.247104
129.738484	4484.207472	24.252122
129.220849	4487.279642	24.257139
129.785977	4504.331861	24.262157
130.228066	4513.936934	24.267175
130.435851	4514.101082	24.272192
130.459335	4503.737872	24.277210
130.433107	4509.817449	24.282227
130.642344	4492.463930	24.287245
130.804023	4499.935490	24.292263
131.082764	4509.713302	24.297280
131.538773	4525.838553	24.302298
131.225149	4533.343146	24.307315
131.644653	4514.624618	24.312333
131.602176	4530.801693	24.317351
131.332252	4521.718777	24.322368
131.827550	4523.313552	24.327386
131.653381	4529.991754	24.332403
131.551339	4523.923345	24.337421
131.804155	4533.091175	24.342439
132.100543	4542.622733	24.347456
132.167900	4550.515522	24.352474
131.948247	4549.515561	24.357491
132.092388	4550.532925	24.362509
132.239778	4568.806565	24.367527
132.273447	4580.670267	24.372544
132.640499	4576.801771	24.377562
132.721545	4592.836388	24.382579
133.173461	4612.297692	24.387597
133.113195	4617.449695	24.392615
133.068943	4618.284041	24.397632
133.396494	4607.889321	24.402650
133.788956	4631.905462	24.407667
133.953047	4627.271190	24.412685
133.812821	4637.727228	24.417703
134.413242	4630.370592	24.422720
134.675085	4627.623654	24.427738
134.393640	4642.373195	24.432755
134.087265	4628.513432	24.437773
134.306625	4627.423454	24.442791
134.511029	4631.601540	24.447808
134.950481	4649.689884	24.452826
134.759300	4663.149448	24.457843
135.108335	4661.853710	24.462861
135.265225	4661.909729	24.467879
135.257907	4658.803333	24.472896
135.464418	4666.332129	24.477914
135.099637	4678.732046	24.482931
135.623921	4678.392525	24.487949
135.737101	4691.219717	24.492967
135.740396	4700.595920	24.497984
135.822573	4708.216990	24.503002
135.977026	4712.284446	24.508019
136.198578	4727.184692	24.513037
136.622591	4740.587359	24.518055
136.563040	4741.622709	24.523072
136.892236	4734.968543	24.528090
136.866586	4758.361051	24.533107
137.136627	4763.623802	24.538125
137.153943	4761.648970	24.543143
137.342630	4765.550898	24.548160
137.700205	4759.463005	24.553178
137.770570	4783.068046	24.558195
137.927879	4789.672574	24.563213
138.271124	4787.426410	24.568231
138.206999	4792.997304	24.573248
138.243266	4785.926954	24.578266
138.298239	4792.480697	24.583283
138.556325	4803.893154	24.588301
138.749643	4819.291177	24.593319
139.136956	4827.672188	24.598336
139.185048	4813.057368	24.603354
139.072895	4824.695740	24.608371
139.096231	4813.599129	24.613389
139.289763	4825.801978	24.618407
139.269514	4844.362014	24.623424
139.638377	4843.676492	24.628442
139.682946	4846.847026	24.633459
139.587430	4852.266414	24.638477
139.894240	4872.197827	24.643495
139.779741	4878.614275	24.648512
140.229049	4870.140577	24.653530
140.491159	4884.397904	24.658547
140.533263	4898.642840	24.663565
140.703320	4893.436516	24.668583
140.783937	4905.020979	24.673600
141.223056	4905.766648	24.678618
141.142754	4929.782761	24.683635
141.445335	4924.052017	24.688653
141.619329	4920.381579	24.693671
141.496362	4928.296618	24.698688
141.820106	4925.129057	24.703706
141.823481	4932.947573	24.708723
142.063707	4952.758589	24.713741
142.140801	4948.300078	24.718759
142.379193	4951.740183	24.723776
142.613915	4944.306125	24.728794
142.350944	4943.171547	24.733811
142.374210	4957.556692	24.738829
142.576134	4975.081459	24.743847
143.027239	4975.865313	24.748864
143.261240	4978.461874	24.753882
143.358764	4979.910699	24.758899
143.392179	4974.767925	24.763917
143.604523	4987.997142	24.768935
143.678228	5001.439128	24.773952
143.949987	4999.489084	24.778970
143.921167	5000.554804	24.783987
143.856195	5001.821040	24.789005
144.417120	5012.392000	24.794023
144.375237	5039.154489	24.799040
144.228873	5028.737934	24.804058
144.472685	5028.439332	24.809075
144.509165	5038.122908	24.814093
144.776981	5041.988965	24.819111
145.134051	5055.200577	24.824128
145.217588	5051.033949	24.829146
145.080494	5064.391966	24.834163
145.424208	5077.893274	24.839181
145.585391	5080.076617	24.844199
145.580374	5091.354851	24.849216
146.012788	5095.896189	24.854234
145.930276	5105.703468	24.859251
146.163926	5103.251733	24.864269
146.468041	5111.488368	24.869287
146.410512	5126.050860	24.874304
146.763399	5123.264350	24.879322
146.610944	5130.690560	24.884339
146.845885	5133.624862	24.889357
147.377836	5150.610036	24.894375
147.438998	5157.207798	24.899392
147.842612	5145.707759	24.904410
147.718478	5157.935894	24.909427
147.611191	5156.288799	24.914445
148.175320	5174.631974	24.919463
148.125555	5184.292903	24.924480
148.406385	5192.865795	24.929498
148.193704	5183.662756	24.934515
148.529647	5189.160466	24.939533
148.900646	5192.291989	24.944551
148.334246	5208.360393	24.949568
148.948024	5208.930671	24.954586
148.873958	5215.195646	24.959603
149.206385	5230.012644	24.964621
149.640072	5231.202640	24.969639
149.288495	5240.307132	24.974656
149.507816	5232.124921	24.979674
149.702925	5251.531088	24.984691
150.099210	5258.324649	24.989709
150.622269	5259.434481	24.994727
150.134750	5270.239842	24.999744
150.603459	5265.447052	25.004762
150.993975	5292.476256	25.009779
150.731170	5291.549546	25.014797
150.944608	5289.730412	25.019815
150.875255	5302.896270	25.024832
151.112793	5293.924999	25.029850
151.125983	5306.503830	25.034867
151.303370	5316.857327	25.039885
151.923212	5316.235772	25.044903
151.699745	5321.773377	25.049920
152.038772	5325.322130	25.054938
152.378714	5344.402786	25.059955
152.199797	5349.943264	25.064973
152.341085	5349.723850	25.069991
152.768293	5335.846758	25.075008
152.764914	5339.537263	25.080026
152.880508	5348.566047	25.085043
152.827800	5367.471524	25.090061
153.176654	5361.400598	25.095079
153.062390	5372.234017	25.100096
153.087288	5373.935118	25.105114
153.308188	5385.550266	25.110131
153.035848	5396.034191	25.115149
153.864241	5413.133602	25.120167
153.814310	5433.895844	25.125184
154.016592	5429.994566	25.130202
154.069018	5435.469206	25.135219
154.109801	5450.285865	25.140237
154.766863	5457.122974	25.145255
154.566919	5476.166371	25.150272
154.982261	5467.669626	25.155290
155.336869	5470.921272	25.160307
155.232391	5479.851887	25.165325
155.521363	5480.416095	25.170343
155.569433	5488.500783	25.175360
155.693143	5490.183175	25.180378
156.070034	5500.211564	25.185395
156.017842	5508.278995	25.190413
156.370334	5504.207125	25.195431
156.081394	5515.097914	25.200448
156.438734	5534.481509	25.205466
156.684742	5523.542071	25.210483
156.561927	5539.827205	25.215501
157.028418	5546.881778	25.220519
157.089102	5567.454185	25.225536
157.324312	5566.333168	25.230554
157.737946	5562.030632	25.235571
157.643383	5565.990681	25.240589
157.970249	5569.472195	25.245607
157.988795	5587.659660	25.250624
158.471327	5587.650744	25.255642
158.653947	5588.653144	25.260659
158.666954	5586.826992	25.265677
158.595173	5577.813835	25.270695
158.729199	5598.339485	25.275712
159.066225	5604.783074	25.280730
159.369640	5610.284743	25.285747
159.240183	5609.819525	25.290765
159.394107	5609.296364	25.295783
159.224281	5625.949305	25.300800
159.813262	5630.636577	25.305818
159.865360	5631.343971	25.310835
159.720101	5643.809111	25.315853
159.883064	5659.593395	25.320871
160.198188	5668.902795	25.325888
160.166519	5671.887641	25.330906
160.486688	5689.831536	25.335923
160.551250	5700.860829	25.340941
160.853250	5704.841107	25.345959
160.881243	5712.866226	25.350976
161.162015	5728.581455	25.355994
161.463234	5723.372047	25.361011
161.706991	5737.399267	25.366029
161.956675	5752.660492	25.371047
161.854615	5767.178177	25.376064
161.968725	5746.067951	25.381082
162.258201	5763.441268	25.386099
162.522014	5775.490662	25.391117
162.811975	5776.968347	25.396135
162.814404	5780.477631	25.401152
162.911219	5781.262691	25.406170
163.392240	5800.161446	25.411187
163.150291	5798.887065	25.416205
163.607493	5798.975283	25.421223
163.807578	5807.517774	25.426240
163.790906	5808.047535	25.431258
164.314121	5794.143122	25.436275
164.155155	5803.749261	25.441293
164.302028	5810.405567	25.446311
164.322665	5828.459069	25.451328
164.305175	5829.909687	25.456346
164.494886	5837.093702	25.461363
164.622310	5851.990908	25.466381
164.816184	5861.327585	25.471399
165.002141	5863.508511	25.476416
165.037623	5875.031062	25.481434
165.467447	5887.721743	25.486451
165.273483	5894.972455	25.491469
165.908376	5897.160974	25.496487
165.769055	5914.985869	25.501504
165.881323	5920.608294	25.506522
165.935117	5914.600185	25.511539
166.324999	5942.326864	25.516557
166.588436	5952.083694	25.521575
166.693386	5960.495521	25.526592
166.629459	5963.996140	25.531610
167.087110	5972.196782	25.536627
167.296425	5983.199945	25.541645
167.126187	5993.123113	25.546663
168.039424	6000.523732	25.551680
167.890164	6009.941721	25.556698
167.934204	6008.179694	25.561715
167.880858	6012.884423	25.566733
168.414363	6030.331052	25.571751
168.403751	6027.902289	25.576768
169.025420	6040.410108	25.581786
169.051485	6049.283988	25.586803
168.815324	6067.475580	25.591821
169.294346	6056.713007	25.596839
169.662131	6063.187923	25.601856
169.580947	6079.106775	25.606874
169.763800	6082.008924	25.611891
169.765373	6090.326092	25.616909
170.240354	6084.252915	25.621927
170.310790	6099.316526	25.626944
170.543008	6117.599972	25.631962
170.731738	6118.621086	25.636979
170.784128	6121.444813	25.641997
170.799471	6117.037942	25.647015
171.122517	6126.506191	25.652032
171.186831	6143.663588	25.657050
171.488612	6133.639174	25.662067
171.526606	6152.690461	25.667085
171.782589	6163.538737	25.672103
171.866583	6175.617419	25.677120
171.980081	6177.307876	25.682138
171.913663	6189.847031	25.687156
172.265702	6199.598797	25.692173
172.248323	6211.891986	25.697191
172.891493	6227.277557	25.702208
172.526146	6235.305837	25.707226
172.865388	6236.838420	25.712244
173.384043	6254.304296	25.717261
173.483426	6255.837210	25.722279
173.738814	6257.376588	25.727296
173.936119	6280.044468	25.732314
174.154769	6277.075987	25.737332
174.384793	6292.946681	25.742349
174.067056	6292.517338	25.747367
174.741134	6285.662868	25.752384
174.714407	6307.170669	25.757402
174.958520	6307.760453	25.762420
174.953663	6322.468915	25.767437
174.963549	6311.965783	25.772455
175.205892	6324.655563	25.777472
175.200375	6351.056663	25.782490
175.486985	6346.952955	25.787508
175.583619	6360.790848	25.792525
175.602674	6375.819121	25.797543
175.808640	6367.652716	25.802560
175.835090	6385.203375	25.807578
176.285077	6390.530614	25.812596
176.705720	6414.144688	25.817613
176.802459	6424.952557	25.822631
177.187808	6423.994085	25.827648
177.065164	6434.892628	25.832666
177.657449	6442.012634	25.837684
177.408277	6452.925836	25.842701
177.607994	6457.422607	25.847719
177.863577	6462.027490	25.852736
178.348126	6481.076131	25.857754
178.530870	6473.463294	25.862772
178.825812	6480.046535	25.867789
178.744262	6478.956631	25.872807
179.065751	6493.201647	25.877824
179.170014	6508.253746	25.882842
179.361821	6502.712483	25.887860
179.557070	6508.396207	25.892877
179.678926	6524.246446	25.897895
180.088652	6522.915314	25.902912
179.984211	6539.747424	25.907930
180.584175	6530.459469	25.912948
180.624562	6539.983427	25.917965
180.418459	6554.109479	25.922983
180.537652	6559.471061	25.928000
180.652235	6564.315134	25.933018
181.076182	6577.992696	25.938036
181.274573	6584.504536	25.943053
180.981568	6596.542771	25.948071
181.539555	6602.338183	25.953088
181.596568	6614.284615	25.958106
181.748341	6621.839952	25.963124
181.706178	6639.919741	25.968141
181.964273	6647.432283	25.973159
182.490826	6656.487510	25.978176
182.813856	6675.751375	25.983194
183.107404	6670.571286	25.988212
182.879175	6690.123346	25.993229
183.361062	6701.895534	25.998247
183.628918	6706.594551	26.003264
183.599282	6708.088219	26.008282
183.958832	6704.263778	26.013300
184.231150	6722.155332	26.018317
184.384368	6736.941192	26.023335
184.552044	6727.906640	26.028352
184.332975	6746.029227	26.033370
184.940119	6755.734378	26.038388
184.994688	6761.329635	26.043405
184.845599	6768.871838	26.048423
185.191802	6765.162228	26.053440
185.220945	6786.455850	26.058458
185.461747	6786.978462	26.063476
185.888234	6801.453700	26.068493
186.039993	6814.144691	26.073511
186.627349	6809.786284	26.078528
186.029925	6823.028225	26.083546
186.459286	6829.001761	26.088564
186.848128	6836.991340	26.093581
186.860293	6839.476858	26.098599
187.135762	6836.159383	26.103616
187.059923	6850.992723	26.108634
187.339153	6875.339008	26.113652
187.339588	6872.132436	26.118669
187.673646	6895.771804	26.123687
187.589317	6894.575996	26.128704
187.679637	6916.557537	26.133722
188.292207	6916.623197	26.138740
188.491003	6935.625174	26.143757
188.563277	6939.297226	26.148775
189.141363	6953.466307	26.153792
188.876263	6959.437500	26.158810
189.071981	6964.109154	26.163828
189.736170	6977.116366	26.168845
189.593378	6993.468525	26.173863
190.139652	6978.426594	26.178880
190.139225	6992.169258	26.183898
190.344160	7011.290035	26.188916
190.448682	7011.915560	26.193933
190.503872	7024.074486	26.198951
190.988588	7027.124543	26.203968
190.803252	7039.775426	26.208986
191.097552	7044.330748	26.214004
191.429870	7064.711260	26.219021
191.412385	7080.357485	26.224039
191.855145	7082.332232	26.229056
192.031722	7101.005685	26.234074
192.139309	7107.043626	26.239092
192.617410	7099.691938	26.244109
192.321510	7130.291890	26.249127
192.606547	7129.094779	26.254144
192.953773	7136.629032	26.259162
193.061732	7154.236363	26.264180
193.559241	7155.473452	26.269197
193.290842	7168.825832	26.274215
193.850765	7173.668044	26.279232
194.098095	7198.795973	26.284250
194.212530	7195.579915	26.289268
194.527559	7204.972946	26.294285
194.599038	7218.154099	26.299303
194.743825	7225.137447	26.304320
194.856974	7237.917089	26.309338
195.182352	7255.575971	26.314356
195.340347	7253.723262	26.319373
195.257966	7253.560546	26.324391
195.491778	7275.710236	26.329408
195.770745	7286.430235	26.334426
196.090683	7297.488466	26.339444
196.351932	7305.842837	26.344461
196.068201	7306.664194	26.349479
196.556336	7313.656906	26.354496
196.884207	7328.341147	26.359514
196.974382	7341.451566	26.364532
197.368935	7364.769693	26.369549
197.418477	7370.486514	26.374567
197.707610	7368.203270	26.379584
198.067027	7392.400803	26.384602
198.060460	7397.569237	26.389620
198.409837	7396.594612	26.394637
198.627826	7404.254364	26.399655
198.371826	7422.275131	26.404672
198.781163	7426.870597	26.409690
198.906474	7436.711077	26.414708
199.450064	7447.969483	26.419725
199.399644	7445.671549	26.424743
199.463306	7461.442561	26.429760
199.911174	7472.951565	26.434778
200.263721	7479.471337	26.439796
200.530137	7476.654630	26.444813
200.471150	7479.994074	26.449831
200.672711	7496.744242	26.454848
201.010999	7495.818709	26.459866
200.812245	7509.308719	26.464884
201.396591	7509.589375	26.469901
201.217808	7522.990231	26.474919
201.387945	7531.323571	26.479936
201.508068	7540.726226	26.484954
201.784751	7554.603095	26.489972
202.163852	7559.527351	26.494989
201.992322	7579.178241	26.500007
202.312590	7582.731404	26.505024
202.602772	7599.145626	26.510042
202.998303	7609.988334	26.515060
203.596542	7619.561586	26.520077
203.211693	7632.134112	26.525095
203.786028	7650.150797	26.530112
203.782880	7649.658303	26.535130
203.882534	7654.320071	26.540148
204.089426	7679.602755	26.545165
204.353380	7690.264072	26.550183
204.556305	7696.174600	26.555200
204.858431	7713.814211	26.560218
204.880047	7712.517304	26.565236
205.332175	7717.594939	26.570253
205.538875	7731.197610	26.575271
205.728011	7733.099424	26.580288
206.245872	7746.341027	26.585306
206.341434	7754.649019	26.590324
206.649918	7758.828827	26.595341
206.630298	7763.659250	26.600359
206.970196	7771.805495	26.605376
207.355410	7783.290438	26.610394
207.372223	7786.717437	26.615412
207.710884	7782.372373	26.620429
207.303715	7802.409928	26.625447
207.825433	7810.452836	26.630464
208.423955	7816.111231	26.635482
208.162122	7819.800199	26.640500
208.281222	7829.483620	26.645517
208.672901	7844.427962	26.650535
208.999891	7847.553132	26.655552
209.049003	7870.848843	26.660570
208.962280	7875.658111	26.665588
209.452328	7885.556645	26.670605
209.394394	7904.857501	26.675623
209.615875	7910.758736	26.680640
210.233171	7925.019088	26.685658
210.210909	7934.650353	26.690676
210.529815	7943.962835	26.695693
210.365976	7964.241525	26.700711
210.614694	7976.132037	26.705728
210.874710	7987.986815	26.710746
211.014663	7997.848062	26.715764
211.376760	8016.274466	26.720781
211.560140	8030.740660	26.725799
211.796437	8046.446649	26.730816
212.461423	8057.108780	26.735834
212.321834	8064.587790	26.740852
212.612694	8075.053495	26.745869
212.765061	8082.709471	26.750887
213.296814	8096.806901	26.755904
213.186761	8105.991196	26.760922
213.080187	8125.389384	26.765940
213.292016	8130.757431	26.770957
213.486065	8146.781665	26.775975
213.926460	8157.537760	26.780992
214.260744	8173.894861	26.786010
214.208053	8184.768839	26.791028
214.583110	8193.468769	26.796045
214.846934	8196.690328	26.801063
214.863428	8208.105857	26.806080
215.237200	8212.527839	26.811098
215.305267	8226.424864	26.816116
216.026960	8235.961511	26.821133
215.771639	8250.041280	26.826151
215.807357	8261.226008	26.831168
216.354325	8268.568613	26.836186
216.407906	8288.129542	26.841204
216.655363	8300.987057	26.846221
216.822661	8302.790937	26.851239
216.974983	8324.569585	26.856256
217.386180	8333.440851	26.861274
217.523655	8356.484745	26.866292
218.193738	8358.341676	26.871309
218.003525	8360.615947	26.876327
218.180289	8377.614558	26.881344
218.837628	8389.844208	26.886362
219.113908	8395.435634	26.891380
219.474718	8413.605120	26.896397
219.446687	8419.842465	26.901415
219.604553	8427.479579	26.906432
219.980676	8431.230077	26.911450
219.908817	8453.264218	26.916468
220.286255	8450.553428	26.921485
220.413722	8460.346131	26.926503
220.291116	8477.685872	26.931520
220.527393	8481.309074	26.936538
220.573538	8500.645411	26.941556
220.864465	8516.618531	26.946573
221.358835	8541.096390	26.951591
221.554846	8549.533114	26.956608
221.963706	8562.761146	26.961626
221.911086	8582.624394	26.966644
222.045978	8597.453616	26.971661
222.751102	8611.385734	26.976679
222.431822	8624.488579	26.981696
222.888572	8630.299142	26.986714
223.347543	8641.366016	26.991732
223.325351	8652.325854	26.996749
223.787032	8664.877212	27.001767
223.758456	8674.495001	27.006784
224.124874	8689.930364	27.011802
224.347599	8700.204519	27.016820
224.453774	8708.735762	27.021837
224.740603	8725.659805	27.026855
224.754509	8732.696205	27.031872
224.974755	8753.752848	27.036890
225.309886	8772.532781	27.041908
225.622518	8774.951529	27.046925
225.997049	8778.740974	27.051943
226.450072	8804.421902	27.056960
226.711422	8810.462607	27.061978
226.497675	8823.314178	27.066996
226.518419	8839.468631	27.072013
227.171966	8841.847496	27.077031
227.133986	8859.165764	27.082048
227.434518	8867.310424	27.087066
227.858795	8894.241710	27.092084
227.874386	8900.482262	27.097101
228.401742	8905.669932	27.102119
228.044289	8911.932854	27.107136
228.621788	8929.917382	27.112154
228.849330	8942.802344	27.117172
229.071831	8948.795177	27.122189
229.288598	8964.755026	27.127207
229.105592	8968.544644	27.132224
229.695766	8978.986602	27.137242
229.899733	8998.374615	27.142260
230.057157	9003.662946	27.147277
230.231148	9010.992014	27.152295
230.373715	9038.631907	27.157312
230.833304	9037.139498	27.162330
230.934737	9061.003355	27.167348
231.358095	9068.905633	27.172365
231.848795	9083.346327	27.177383
231.903724	9086.505753	27.182400
232.462645	9096.095863	27.187418
232.658300	9117.385511	27.192436
232.343536	9118.190821	27.197453
232.840409	9124.081579	27.202471
232.833232	9154.920415	27.207488
233.215129	9156.035012	27.212506
233.137888	9167.216227	27.217524
233.523423	9171.122900	27.222541
233.980227	9184.401808	27.227559
234.081888	9207.445767	27.232576
234.320591	9207.901854	27.237594
234.626411	9235.355929	27.242612
234.506127	9233.996522	27.247629
234.959655	9258.150585	27.252647
235.371133	9272.731399	27.257664
235.685197	9282.110065	27.262682
235.630774	9297.515634	27.267700
235.547774	9310.555501	27.272717
236.171129	9329.513682	27.277735
236.073322	9346.945580	27.282752
236.677583	9352.048190	27.287770
236.694044	9374.375424	27.292788
237.144134	9399.915992	27.297805
237.323465	9404.114466	27.302823
237.627961	9425.600784	27.307840
238.030146	9425.531931	27.312858
238.401283	9447.279823	27.317876
238.542382	9447.775709	27.322893
239.369771	9458.748289	27.327911
239.088305	9480.295444	27.332928
239.350420	9470.996346	27.337946
239.622613	9495.607771	27.342964
239.810787	9507.329042	27.347981
240.124332	9510.002212	27.352999
240.192258	9522.372848	27.358016
240.349931	9536.559478	27.363034
240.723543	9546.902160	27.368052
240.737554	9573.102102	27.373069
241.310894	9571.588454	27.378087
241.423875	9582.119258	27.383104
241.581737	9598.257291	27.388122
241.892720	9612.320922	27.393140
241.934495	9626.633958	27.398157
242.348142	9639.710834	27.403175
242.328000	9646.604377	27.408192
242.589725	9657.065702	27.413210
242.960079	9675.064879	27.418228
242.930841	9691.109504	27.423245
243.333688	9694.847215	27.428263
243.368722	9721.768700	27.433280
243.669807	9742.692727	27.438298
243.940707	9751.390271	27.443316
244.085765	9777.032354	27.448333
244.417633	9781.974578	27.453351
244.804436	9803.480867	27.458368
245.128263	9812.304397	27.463386
245.228706	9830.180625	27.468404
245.565804	9854.027920	27.473421
245.945567	9854.908154	27.478439
246.032827	9865.772708	27.483456
246.543047	9883.278640	27.488474
246.273669	9892.720371	27.493492
246.632515	9916.033958	27.498509
246.889448	9914.444244	27.503527
247.140590	9938.556418	27.508544
247.502023	9951.405060	27.513562
248.006557	9968.752100	27.518580
247.906400	9981.590517	27.523597
248.183314	9991.247547	27.528615
248.489960	10014.298120	27.533632
248.709635	10027.008786	27.538650
249.121831	10037.999290	27.543668
248.879038	10050.747139	27.548685
249.377495	10066.130462	27.553703
249.671469	10087.305855	27.558720
249.641576	10107.535927	27.563738
250.053647	10125.586214	27.568756
250.404355	10152.939101	27.573773
250.319854	10144.131089	27.578791
250.841496	10169.582256	27.583808
251.069467	10189.687809	27.588826
251.413565	10203.267477	27.593844
251.038978	10224.080237	27.598861
251.768235	10244.908829	27.603879
252.417408	10263.167401	27.608896
252.590941	10275.219395	27.613914
252.986868	10289.956550	27.618932
252.684817	10301.621680	27.623949
253.557076	10328.550549	27.628967
253.741733	10334.768397	27.633984
254.038525	10362.545756	27.639002
254.035960	10363.723297	27.644020
253.987851	10388.397778	27.649037
254.801598	10398.919472	27.654055
255.145506	10423.178524	27.659072
254.951510	10428.087459	27.664090
255.472324	10443.956693	27.669108
255.770777	10458.522632	27.674125
256.527631	10478.769472	27.679143
256.328037	10480.022182	27.684160
256.620176	10493.778507	27.689178
256.935385	10506.593490	27.694196
256.905561	10523.045568	27.699213
257.529395	10534.055740	27.704231
257.630270	10544.103078	27.709248
257.775976	10557.286510	27.714266
258.157035	10572.852837	27.719284
258.454191	10590.350693	27.724301
258.895471	10594.678656	27.729319
259.019908	10616.615511	27.734336
259.397774	10616.103974	27.739354
259.529220	10631.253149	27.744372
259.571840	10653.554978	27.749389
259.423628	10643.701518	27.754407
259.964776	10670.302876	27.759424
259.877819	10688.682214	27.764442
260.632332	10700.526478	27.769460
261.105104	10719.429298	27.774477
260.987436	10739.625843	27.779495
261.264714	10743.334954	27.784512
261.649487	10762.228756	27.789530
262.271593	10770.456666	27.794548
261.873685	10800.059427	27.799565
262.316816	10799.362177	27.804583
262.679587	10817.103108	27.809600
262.777664	10836.025545	27.814618
262.894377	10836.932838	27.819636
263.184721	10864.125960	27.824653
263.616653	10872.257770	27.829671
264.096133	10892.347779	27.834688
263.958690	10905.614609	27.839706
264.656024	10919.165560	27.844724
264.835459	10932.036448	27.849741
264.897927	10928.260199	27.854759
264.926593	10951.426674	27.859776
265.140820	10966.997364	27.864794
265.646476	10985.920265	27.869812
265.520530	11003.643030	27.874829
266.270192	11019.044774	27.879847
266.268364	11045.935177	27.884864
266.462839	11066.203368	27.889882
267.306708	11075.414234	27.894900
267.162460	11101.064556	27.899917
267.607149	11121.824001	27.904935
267.598004	11130.416590	27.909952
267.764617	11157.767778	27.914970
268.396328	11168.246055	27.919988
268.504526	11192.600435	27.925005
268.811943	11205.600052	27.930023
269.345597	11211.502833	27.935040
269.401714	11231.247346	27.940058
269.713803	11242.758703	27.945076
269.992842	11265.220787	27.950093
270.509085	11277.388559	27.955111
270.963871	11299.950811	27.960128
270.932186	11306.761882	27.965146
271.166414	11322.542332	27.970164
271.878344	11341.653690	27.975181
271.579183	11347.770017	27.980199
271.943431	11362.186427	27.985216
272.285945	11384.461682	27.990234
272.473610	11397.492308	27.995252
272.469160	11412.864835	28.000269
272.866660	11432.798905	28.005287
273.199439	11459.765396	28.010304
273.278696	11485.814246	28.015322
273.733274	11488.421072	28.020340
274.231141	11517.429338	28.025357
274.376315	11531.281788	28.030375
274.784457	11541.964351	28.035392
275.128235	11563.930790	28.040410
275.571931	11579.200929	28.045428
275.783773	11590.420273	28.050445
276.029489	11601.263705	28.055463
276.530419	11619.253686	28.060480
276.335062	11632.894706	28.065498
276.817331	11646.740304	28.070516
277.215646	11658.748245	28.075533
277.403676	11674.747844	28.080551
277.514121	11691.395351	28.085568
277.654857	11704.949281	28.090586
277.957884	11715.203406	28.095604
278.265060	11743.288704	28.100621
278.430367	11758.743766	28.105639
278.924879	11784.711752	28.110656
278.947983	11798.263170	28.115674
279.344846	11814.874423	28.120692
279.639969	11840.623373	28.125709
280.040819	11853.751447	28.130727
280.163966	11868.884246	28.135744
280.482316	11882.760332	28.140762
280.815850	11896.309297	28.145780
281.040427	11922.423040	28.150797
280.982039	11929.443648	28.155815
281.448009	11942.770600	28.160832
281.897311	11958.037018	28.165850
281.883368	11983.481217	28.170868
282.220010	11996.319050	28.175885
282.750017	12019.952456	28.180903
282.967095	12027.726458	28.185920
283.444871	12050.325349	28.190938
283.584013	12052.886782	28.195956
283.497963	12078.979706	28.200973
283.880594	12085.547602	28.205991
284.394528	12106.071504	28.211008
284.511427	12141.696316	28.216026
284.956518	12143.871464	28.221044
285.276695	12167.610731	28.226061
285.456623	12177.053477	28.231079
285.661193	12192.604884	28.236096
285.736390	12220.822383	28.241114
285.781918	12235.856487	28.246132
286.320056	12262.041789	28.251149
286.608378	12284.059357	28.256167
286.952556	12304.978787	28.261184
287.032404	12327.588779	28.266202
288.025455	12355.452870	28.271220
288.113768	12372.265477	28.276237
287.865279	12395.156837	28.281255
288.006222	12422.147229	28.286272
288.390086	12439.960517	28.291290
289.130262	12457.595078	28.296308
289.697435	12484.526052	28.301325
289.570112	12499.678836	28.306343
290.478640	12515.717591	28.311360
290.613850	12535.425383	28.316378
291.200909	12561.782723	28.321396
291.794981	12562.663103	28.326413
291.750821	12584.376810	28.331431
292.165999	12582.710221	28.336448
292.666295	12602.214257	28.341466
292.642964	12613.772658	28.346484
293.091903	12628.518148	28.351501
293.073046	12640.164076	28.356519
293.561656	12657.415005	28.361536
293.572798	12674.719772	28.366554
293.689513	12691.308958	28.371572
293.759415	12700.404613	28.376589
293.515693	12718.775950	28.381607
294.231971	12743.585145	28.386624
294.554232	12772.181896	28.391642
295.275930	12791.022299	28.396660
295.945732	12807.037823	28.401677
295.810699	12833.067570	28.406695
296.287903	12838.063116	28.411712
296.711511	12861.973811	28.416730
296.738704	12879.238317	28.421748
296.927214	12897.101779	28.426765
297.156196	12918.813269	28.431783
298.142289	12942.298457	28.436800
298.120384	12947.702870	28.441818
298.558184	12973.597048	28.446836
298.567371	12991.948892	28.451853
298.377668	13008.166771	28.456871
298.988492	13021.399718	28.461888
299.197249	13043.571744	28.466906
299.476022	13068.912453	28.471924
299.800387	13082.996595	28.476941
299.955109	13100.626330	28.481959
300.453418	13117.428576	28.486976
300.601837	13138.699824	28.491994
300.991284	13150.496012	28.497012
301.133227	13170.877964	28.502029
301.124447	13196.167184	28.507047
302.161287	13213.082109	28.512064
302.430505	13224.315150	28.517082
302.501837	13241.312700	28.522100
302.674852	13249.918807	28.527117
302.757055	13276.961314	28.532135
303.250132	13295.313777	28.537152
303.425055	13324.192767	28.542170
303.794626	13345.826397	28.547188
304.195628	13369.996887	28.552205
304.427100	13389.867864	28.557223
305.020543	13401.356250	28.562240
305.176565	13420.060927	28.567258
305.410264	13441.671471	28.572276
305.588576	13474.203274	28.577293
305.486885	13502.256849	28.582311
306.112429	13516.069302	28.587328
306.460477	13551.156195	28.592346
306.960664	13569.775708	28.597364
307.620328	13598.029654	28.602381
307.569898	13616.940512	28.607399
307.742786	13639.484915	28.612416
308.188435	13669.821625	28.617434
308.513726	13684.126774	28.622452
309.076988	13707.022717	28.627469
309.131537	13728.688511	28.632487
309.689286	13750.835251	28.637504
309.961931	13772.870036	28.642522
310.244569	13800.849476	28.647540
310.933307	13812.229396	28.652557
310.498778	13830.539001	28.657575
311.274349	13848.689304	28.662592
311.666984	13874.861889	28.667610
311.847487	13900.730784	28.672628
312.250475	13916.490550	28.677645
312.279705	13940.419251	28.682663
312.457344	13955.612738	28.687680
313.159103	13980.024339	28.692698
313.168655	14005.013904	28.697716
314.076104	14012.182865	28.702733
313.886834	14040.180937	28.707751
314.436093	14056.846486	28.712768
314.784856	14073.146501	28.717786
315.091452	14100.782065	28.722804
315.568094	14121.250070	28.727821
315.511153	14147.147625	28.732839
316.204319	14155.047153	28.737856
316.301353	14185.667899	28.742874
316.777858	14202.195915	28.747892
317.003804	14218.645641	28.752909
317.144993	14243.867526	28.757927
317.122588	14264.881672	28.762944
317.796815	14285.351851	28.767962
318.039752	14300.662511	28.772980
318.393771	14325.144796	28.777997
319.030445	14342.456537	28.783015
319.118936	14358.867689	28.788032
319.564955	14377.668882	28.793050
319.500009	14409.462656	28.798068
319.995934	14417.667620	28.803085
320.280917	14449.950447	28.808103
320.645633	14475.485577	28.813120
321.133822	14496.535288	28.818138
321.232505	14512.840886	28.823156
321.605699	14525.055271	28.828173
321.911286	14552.482146	28.833191
322.139603	14565.831677	28.838208
322.395414	14592.956371	28.843226
322.647480	14612.815968	28.848244
323.307377	14634.904447	28.853261
323.583226	14644.772477	28.858279
323.629002	14676.382951	28.863296
323.997873	14691.003292	28.868314
324.339616	14711.740236	28.873332
324.964964	14738.419436	28.878349
325.124851	14758.327566	28.883367
325.318717	14781.706978	28.888384
325.678747	14802.059592	28.893402
325.507641	14829.994534	28.898420
326.241057	14852.375326	28.903437
326.617971	14873.029423	28.908455
327.126676	14899.126118	28.913472
327.068976	14921.855454	28.918490
327.290173	14945.684497	28.923508
327.959478	14957.859649	28.928525
327.932963	15002.353312	28.933543
328.364775	15020.032243	28.938560
329.074690	15045.451231	28.943578
329.305266	15079.195915	28.948596
329.344397	15098.992050	28.953613
329.688356	15130.448440	28.958631
330.485839	15152.122387	28.963648
330.692837	15172.549651	28.968666
330.578053	15193.261893	28.973684
331.241578	15228.914858	28.978701
331.828698	15249.332889	28.983719
332.294449	15266.727490	28.988736
332.714025	15283.951648	28.993754
332.758313	15313.989018	28.998772
333.291937	15327.121563	29.003789
333.538017	15359.593875	29.008807
333.717852	15374.372208	29.013824
334.353815	15392.533154	29.018842
334.384671	15414.644843	29.023860
335.087300	15423.024155	29.028877
335.179514	15456.335426	29.033895
335.525160	15478.704026	29.038912
336.037037	15496.363914	29.043930
336.148140	15523.422677	29.048948
336.807758	15540.106149	29.053965
336.676352	15577.371474	29.058983
336.990034	15595.932748	29.064000
337.433926	15614.995783	29.069018
337.615700	15650.489821	29.074036
337.754268	15662.617794	29.079053
337.840575	15690.981290	29.084071
338.305313	15731.346379	29.089088
338.833888	15753.595232	29.094106
339.216824	15787.856784	29.099124
339.664214	15811.534580	29.104141
339.913204	15833.541372	29.109159
340.206200	15861.087577	29.114176
340.727400	15892.282808	29.119194
340.694027	15922.244296	29.124212
341.184881	15943.501907	29.129229
341.499979	15974.471332	29.134247
341.905365	15994.858898	29.139264
342.400110	16019.972972	29.144282
342.599281	16050.525114	29.149300
343.157443	16077.815002	29.154317
343.335032	16111.353050	29.159335
343.896993	16126.819095	29.164352
344.365453	16148.789982	29.169370
344.486121	16162.964084	29.174388
344.949960	16182.992285	29.179405
345.450941	16208.417708	29.184423
345.390097	16226.636589	29.189440
346.402489	16244.911138	29.194458
346.392199	16269.295841	29.199476
346.790064	16274.414346	29.204493
346.951431	16292.752569	29.209511
347.197192	16316.314719	29.214528
347.612626	16342.269942	29.219546
347.461851	16371.963221	29.224564
348.410229	16386.109279	29.229581
348.584401	16423.234507	29.234599
348.892195	16446.918982	29.239616
349.263483	16468.668364	29.244634
349.266238	16496.455972	29.249652
349.969608	16514.674783	29.254669
350.085560	16540.473395	29.259687
350.427897	16570.782125	29.264704
351.132241	16598.397036	29.269722
351.320953	16637.145479	29.274740
351.879556	16659.179364	29.279757
352.340963	16686.918175	29.284775
352.341860	16710.171480	29.289792
352.745039	16731.707859	29.294810
352.846872	16769.955546	29.299828
353.307922	16793.446488	29.304845
353.548063	16825.858038	29.309863
353.600995	16857.829322	29.314880
354.439090	16883.497910	29.319898
354.758398	16931.937033	29.324916
355.397631	16948.942149	29.329933
355.617417	16984.716494	29.334951
356.051998	17007.580020	29.339968
356.397046	17024.853013	29.344986
356.469206	17056.134224	29.350004
356.863290	17085.074967	29.355021
357.465065	17109.635458	29.360039
357.830244	17143.067307	29.365056
358.220742	17171.695106	29.370074
358.272623	17201.268051	29.375092
359.152784	17225.393283	29.380109
359.246172	17264.141628	29.385127
359.500200	17291.824349	29.390144
360.014558	17315.427011	29.395162
360.327501	17345.723108	29.400180
360.684092	17367.091475	29.405197
361.123495	17386.984885	29.410215
361.062929	17428.263915	29.415232
361.952398	17446.298472	29.420250
362.129838	17478.338620	29.425268
362.719711	17510.416183	29.430285
362.947262	17535.400231	29.435303
363.464009	17566.905176	29.440320
363.717371	17585.220144	29.445338
363.808576	17609.224299	29.450356
364.300442	17633.211042	29.455373
364.791940	17660.473592	29.460391
365.239003	17688.430842	29.465408
365.674948	17710.705547	29.470426
366.053640	17737.755166	29.475444
366.322090	17763.736944	29.480461
366.625558	17798.982138	29.485479
366.978027	17817.509536	29.490496
367.550680	17847.419910	29.495514
367.714166	17868.174561	29.500532
368.214801	17892.634724	29.505549
368.734750	17905.412174	29.510567
368.705600	17940.955486	29.515584
369.090741	17944.022566	29.520602
369.060207	17986.138231	29.525620
369.633250	18009.397970	29.530637
370.229094	18030.071805	29.535655
370.437776	18064.806729	29.540672
370.828776	18080.575623	29.545690
370.824579	18127.210024	29.550708
370.896151	18148.208818	29.555725
371.516062	18176.370015	29.560743
371.788471	18217.141877	29.565760
372.307058	18241.268532	29.570778
372.639163	18276.287719	29.575796
373.149229	18318.921677	29.580813
373.808103	18348.465560	29.585831
373.860258	18378.113066	29.590848
374.404932	18406.509384	29.595866
374.991227	18430.812705	29.600884
375.227938	18466.075088	29.605901
375.481787	18497.265876	29.610919
375.996458	18528.621647	29.615936
376.371512	18563.298543	29.620954
377.084818	18596.204333	29.625972
377.071166	18615.296108	29.630989
377.721465	18647.469912	29.636007
377.607814	18687.196984	29.641024
378.615509	18706.658978	29.646042
378.995123	18732.677469	29.651060
379.062125	18765.881317	29.656077
379.617175	18796.800530	29.661095
379.621959	18821.359889	29.666112
379.950133	18849.573663	29.671130
380.506299	18895.746990	29.676148
380.830004	18929.936551	29.681165
381.149762	18968.988760	29.686183
381.562387	19002.531576	29.691200
382.024432	19027.836917	29.696218
382.044133	19074.540947	29.701236
382.715140	19105.573967	29.706253
383.286397	19137.845354	29.711271
383.484665	19170.807567	29.716288
384.042479	19204.115504	29.721306
384.125877	19234.374199	29.726324
384.483096	19265.420037	29.731341
384.920728	19306.793094	29.736359
385.423291	19348.071951	29.741376
385.881682	19386.441621	29.746394
386.612167	19413.360061	29.751412
386.234427	19448.250094	29.756429
386.757219	19478.062866	29.761447
387.266845	19519.834436	29.766464
387.827131	19551.815199	29.771482
388.310781	19586.283903	29.776500
388.483797	19618.202764	29.781517
389.283541	19647.597933	29.786535
389.554001	19696.325914	29.791552
390.098008	19727.891917	29.796570
390.631492	19743.600966	29.801588
390.785427	19777.744680	29.806605
391.540245	19802.827739	29.811623
391.644648	19835.630216	29.816640
391.957739	19849.338897	29.821658
392.265166	19882.017999	29.826676
393.017064	19910.097216	29.831693
393.611619	19942.765177	29.836711
393.926097	19960.292225	29.841728
394.154130	19989.889824	29.846746
394.532343	20005.941713	29.851764
394.621267	20030.555134	29.856781
395.263682	20051.289988	29.861799
395.129309	20079.727435	29.866816
395.939271	20101.361665	29.871834
396.522068	20135.239629	29.876852
396.637352	20165.783245	29.881869
396.971953	20194.223676	29.886887
397.309223	20229.488894	29.891904
397.431558	20255.743104	29.896922
398.331456	20277.618091	29.901940
397.945514	20314.029561	29.906957
398.725187	20349.931295	29.911975
399.006611	20388.625800	29.916992
399.562534	20419.926259	29.922010
400.022784	20445.634506	29.927028
400.140982	20482.156829	29.932045
400.763439	20513.664029	29.937063
401.161234	20539.069003	29.942080
401.351703	20579.888555	29.947098
402.033125	20616.680585	29.952116
402.258618	20657.656925	29.957133
402.791643	20685.470947	29.962151
403.303136	20731.046553	29.967168
403.567686	20759.679273	29.972186
404.203819	20790.625012	29.977204
404.551807	20832.210594	29.982221
405.191035	20861.349081	29.987239
405.347499	20891.685383	29.992256
405.646405	20931.721574	29.997274
406.034607	20961.609710	30.002292
406.489707	20997.546048	30.007309
407.283810	21027.950502	30.012327
407.385796	21064.112551	30.017344
408.044715	21082.293278	30.022362
408.302075	21122.792464	30.027380
408.764725	21165.359520	30.032397
409.283640	21189.490373	30.037415
409.449331	21224.393470	30.042432
409.622988	21266.247057	30.047450
410.237944	21298.788140	30.052468
410.087226	21338.388851	30.057485
410.796672	21369.378705	30.062503
411.191268	21409.419112	30.067520
411.407932	21448.449995	30.072538
412.428143	21482.512133	30.077556
412.709118	21530.717050	30.082573
413.339437	21563.014859	30.087591
413.565471	21600.480413	30.092608
413.893008	21627.691417	30.097626
414.729647	21671.385146	30.102644
415.077636	21701.815768	30.107661
415.269816	21732.559201	30.112679
415.803064	21760.739193	30.117696
416.159817	21800.592847	30.122714
416.838354	21827.787080	30.127732
417.241176	21864.017732	30.132749
417.619237	21891.890927	30.137767
417.804390	21926.412248	30.142784
418.191840	21963.240101	30.147802
418.675124	22003.041756	30.152820
418.663248	22028.873127	30.157837
418.925357	22069.077355	30.162855
419.856966	22112.297661	30.167872
420.232058	22153.311208	30.172890
420.661579	22176.116411	30.177908
420.871171	22215.334717	30.182925
421.312024	22243.351048	30.187943
421.931336	22277.351842	30.192960
422.120424	22308.956193	30.197978
422.717616	22332.199017	30.202996
423.173707	22369.424788	30.208013
423.595569	22397.772496	30.213031
424.131231	22435.125580	30.218048
424.206601	22472.791446	30.223066
424.646379	22496.375913	30.228084
424.994699	22549.197421	30.233101
425.611710	22580.472857	30.238119
425.981196	22607.143944	30.243136
426.483106	22647.372930	30.248154
426.929593	22683.820443	30.253172
427.279606	22732.807350	30.258189
427.771918	22758.013951	30.263207
427.714929	22791.295121	30.268224
428.104905	22835.043699	30.273242
428.761417	22862.115513	30.278260
428.935453	22919.256084	30.283277
429.525413	22946.462043	30.288295
430.378804	22989.836297	30.293312
430.666063	23039.761677	30.298330
431.508437	23063.229843	30.303348
431.409675	23105.292314	30.308365
432.057852	23141.177595	30.313383
432.744766	23180.718086	30.318400
433.086850	23219.517827	30.323418
433.702388	23250.034677	30.328436
433.829975	23291.240159	30.333453
434.433124	23325.985296	30.338471
434.997022	23355.621506	30.343488
435.562076	23384.469121	30.348506
436.049271	23421.463396	30.353524
436.139658	23457.168848	30.358541
436.746933	23494.468255	30.363559
437.149649	23531.736943	30.368576
437.367975	23557.117803	30.373594
437.864060	23607.347748	30.378612
438.208936	23649.607795	30.383629
438.582681	23679.141998	30.388647
438.819287	23723.348742	30.393664
439.400391	23760.351866	30.398682
439.674913	23797.150341	30.403700
440.236693	23852.884731	30.408717
440.629738	23892.830324	30.413735
441.069463	23935.269347	30.418752
441.640797	23983.729633	30.423770
442.121220	24021.260922	30.428788
442.654807	24066.810294	30.433805
442.694783	24099.768879	30.438823
443.470645	24136.340034	30.443840
443.580359	24187.053524	30.448858
444.678584	24224.082463	30.453876
445.121336	24279.377461	30.458893
445.119912	24313.355738	30.463911
445.904009	24339.707026	30.468928
446.209209	24386.474642	30.473946
446.599781	24422.037809	30.478964
447.044970	24469.652994	30.483981
447.586409	24507.806057	30.488999
447.859477	24544.912322	30.494016
448.041601	24592.233899	30.499034
448.708413	24621.090420	30.504052
449.057130	24673.235583	30.509069
449.473111	24712.516941	30.514087
450.033099	24756.313271	30.519104
450.547812	24800.284373	30.524122
451.532137	24832.659130	30.529140
451.717994	24869.215947	30.534157
451.934073	24898.831967	30.539175
452.263196	24934.633462	30.544192
452.561165	24978.467413	30.549210
453.484575	25007.550222	30.554228
453.911942	25045.906301	30.559245
454.118868	25080.441438	30.564263
454.528042	25118.706066	30.569280
454.895942	25168.348323	30.574298
455.405880	25196.235063	30.579316
456.297551	25236.498696	30.584333
456.536044	25276.451012	30.589351
456.963094	25311.782887	30.594368
457.308994	25365.028270	30.599386
457.903865	25399.660711	30.604404
458.077673	25439.138363	30.609421
458.370952	25477.306263	30.614439
459.147377	25520.176085	30.619456
459.269469	25573.739876	30.624474
459.834191	25612.973444	30.629492
460.151821	25660.458482	30.634509
460.748228	25713.404839	30.639527
461.274073	25747.118899	30.644544
461.633361	25802.637639	30.649562
462.178729	25838.752200	30.654580
462.760540	25883.289047	30.659597
463.060154	25935.695352	30.664615
463.839364	25974.380099	30.669632
464.248451	26019.851166	30.674650
464.560885	26057.313771	30.679668
464.984857	26107.416294	30.684685
465.310172	26167.575532	30.689703
466.027014	26211.396927	30.694720
466.158464	26254.148198	30.699738
466.594261	26308.725372	30.704756
467.319336	26349.353543	30.709773
467.705231	26396.561188	30.714791
468.404890	26448.205729	30.719808
468.536718	26496.783688	30.724826
468.898982	26545.743185	30.729844
469.590031	26593.812493	30.734861
470.278467	26645.364848	30.739879
471.031941	26698.474346	30.744896
471.290131	26740.278442	30.749914
471.974501	26775.138575	30.754932
472.779656	26821.429453	30.759949
472.847692	26876.807420	30.764967
473.435389	26915.043337	30.769984
473.984772	26954.250950	30.775002
474.497209	26993.795986	30.780020
474.955317	27025.637372	30.785037
475.116199	27085.369610	30.790055
475.863634	27117.283157	30.795072
476.096139	27164.758023	30.800090
476.935712	27202.744697	30.805108
477.367967	27250.101569	30.810125
477.627952	27293.679549	30.815143
478.144733	27332.896569	30.820160
478.599320	27380.963030	30.825178
479.238791	27423.775073	30.830196
479.940085	27463.586458	30.835213
480.022582	27503.137558	30.840231
480.357321	27541.233752	30.845248
480.957640	27593.648941	30.850266
481.175445	27633.026525	30.855284
482.107378	27672.311259	30.860301
482.447811	27713.460550	30.865319
483.298279	27752.579135	30.870336
483.526217	27793.400222	30.875354
484.050785	27827.083850	30.880372
484.650636	27852.565636	30.885389
484.767035	27891.124606	30.890407
485.329881	27929.183903	30.895424
485.649650	27975.267959	30.900442
486.046997	28015.427446	30.905460
486.278291	28050.049654	30.910477
486.690189	28106.863644	30.915495
487.289449	28152.444488	30.920512
488.041906	28198.422831	30.925530
488.344418	28245.876445	30.930548
488.940044	28286.420168	30.935565
489.092378	28336.902174	30.940583
489.649464	28378.913129	30.945600
489.861667	28433.035535	30.950618
490.479156	28490.513952	30.955636
491.149341	28543.472523	30.960653
491.585439	28587.627160	30.965671
492.351679	28626.506114	30.970688
492.413864	28684.051822	30.975706
493.039966	28739.851287	30.980724
493.825184	28798.280950	30.985741
494.016490	28848.092319	30.990759
494.996156	28898.006830	30.995776
495.407699	28948.037579	31.000794
495.701212	28992.677441	31.005812
496.264962	29039.660924	31.010829
496.481167	29096.049906	31.015847
497.569002	29149.370265	31.020864
497.954655	29198.339668	31.025882
498.610093	29248.744209	31.030900
498.986802	29286.641669	31.035917
499.531602	29343.642757	31.040935
500.271322	29386.619712	31.045952
500.938163	29430.955986	31.050970
501.051460	29473.598279	31.055988
501.843145	29514.295397	31.061005
502.098742	29560.428958	31.066023
502.555300	29608.334021	31.071040
502.943920	29666.261166	31.076058
503.456530	29708.087070	31.081076
504.179613	29759.986812	31.086093
504.412518	29814.759991	31.091111
504.883157	29867.569448	31.096128
505.806235	29908.965083	31.101146
506.238787	29959.834479	31.106164
506.541681	30006.926822	31.111181
506.911263	30065.726069	31.116199
507.583889	30105.658658	31.121216
508.234022	30156.965878	31.126234
508.611993	30210.738218	31.131252
509.146166	30259.903707	31.136269
509.311329	30314.812701	31.141287
509.806803	30363.603119	31.146304
510.265595	30421.912375	31.151322
510.701329	30479.174987	31.156340
511.356047	30528.993320	31.161357
511.766380	30594.359711	31.166375
512.618188	30627.688539	31.171392
513.387687	30691.052290	31.176410
513.678348	30745.986032	31.181428
514.181153	30784.168754	31.186445
514.385637	30837.725613	31.191463
514.972974	30889.698483	31.196480
515.650821	30944.644500	31.201498
516.189746	30997.682689	31.206516
516.919879	31031.792823	31.211533
517.278147	31093.859863	31.216551
517.900146	31130.436535	31.221568
518.065358	31172.332872	31.226586
518.553584	31231.346708	31.231604
519.093660	31273.859634	31.236621
519.590764	31318.787238	31.241639
519.990431	31362.443730	31.246656
520.367891	31415.115483	31.251674
520.784693	31474.877131	31.256692
521.549143	31528.838807	31.261709
522.068033	31582.516284	31.266727
522.341003	31630.211112	31.271744
522.777560	31694.438165	31.276762
523.202667	31754.742100	31.281780
524.154760	31811.677474	31.286797
524.458807	31868.594051	31.291815
525.119112	31922.350130	31.296832
525.676871	31973.933506	31.301850
526.285718	32031.128328	31.306868
526.958223	32086.085089	31.311885
527.446372	32145.098829	31.316903
528.121344	32206.243315	31.321920
528.587952	32258.552573	31.326938
529.182431	32313.541883	31.331956
529.753104	32362.375865	31.336973
530.005184	32419.511067	31.341991
530.804532	32468.651447	31.347008
531.243187	32534.215957	31.352026
531.550301	32583.627434	31.357044
532.215002	32642.285442	31.362061
532.652115	32702.994517	31.367079
532.853124	32759.299896	31.372096
533.792876	32830.383628	31.377114
534.251484	32883.005290	31.382132
534.883373	32950.126594	31.387149
535.301142	32996.968067	31.392167
535.878251	33060.558313	31.397184
536.864372	33116.921090	31.402202
537.230184	33182.348572	31.407220
537.757443	33229.983528	31.412237
538.443263	33287.235924	31.417255
538.787818	33344.406126	31.422272
539.515121	33390.960745	31.427290
539.739918	33464.825510	31.432308
540.418161	33517.895518	31.437325
540.900485	33572.364504	31.442343
541.726208	33627.856074	31.447360
542.258924	33678.763760	31.452378
542.541279	33747.009366	31.457396
543.070970	33797.065851	31.462413
543.540855	33858.877935	31.467431
543.929781	33905.145914	31.472448
544.775677	33972.967784	31.477466
545.185264	34029.046998	31.482484
545.847932	34097.593923	31.487501
546.293125	34149.318992	31.492519
546.644139	34203.290926	31.497536
547.053314	34271.041024	31.502554
547.872388	34344.334562	31.507572
548.454306	34403.750517	31.512589
549.119819	34452.170587	31.517607
549.687846	34511.526082	31.522624
550.802320	34564.552263	31.527642
550.930797	34625.852278	31.532660
551.834568	34679.630041	31.537677
552.300065	34730.214163	31.542695
552.971217	34784.033886	31.547712
553.382423	34825.055489	31.552730
553.822837	34868.379309	31.557748
554.318025	34917.658819	31.562765
554.891139	34962.936503	31.567783
555.194834	35019.683298	31.572800
556.130154	35062.812085	31.577818
556.436685	35114.944749	31.582836
556.990920	35167.721419	31.587853
557.463053	35215.793680	31.592871
557.820035	35270.200200	31.597888
558.414728	35325.356544	31.602906
558.786961	35387.695009	31.607924
559.458051	35441.810219	31.612941
559.912470	35503.614748	31.617959
560.107912	35563.455115	31.622976
561.049909	35621.310100	31.627994
561.458774	35697.268129	31.633012
562.104819	35745.672817	31.638029
562.972422	35805.393301	31.643047
563.512768	35867.569898	31.648064
563.879988	35925.685080	31.653082
564.544425	35993.273185	31.658100
565.084166	36055.734579	31.663117
565.562920	36117.811765	31.668135
566.141613	36184.136548	31.673152
567.004802	36252.497548	31.678170
567.369522	36310.734315	31.683188
567.785314	36370.626112	31.688205
568.401430	36438.817236	31.693223
568.817154	36500.255995	31.698240
569.318176	36567.169458	31.703258
569.841818	36641.891020	31.708276
570.902397	36713.913860	31.713293
571.352777	36776.452496	31.718311
571.674500	36844.334048	31.723328
572.619923	36907.662347	31.728346
572.945210	36973.189232	31.733364
573.710114	37039.489494	31.738381
574.299272	37099.285576	31.743399
574.754918	37169.058889	31.748416
575.546222	37226.893451	31.753434
575.983286	37293.788614	31.758452
576.555066	37355.927246	31.763469
577.413445	37424.785854	31.768487
577.792591	37497.524262	31.773504
578.433123	37550.063195	31.778522
579.062810	37622.239848	31.783540
579.635954	37681.690140	31.788557
580.521623	37739.305555	31.793575
580.530422	37804.379621	31.798592
581.469299	37867.627131	31.803610
581.847347	37942.365507	31.808628
582.375887	38002.051487	31.813645
583.057378	38069.363586	31.818663
583.588389	38154.111872	31.823680
584.467560	38208.967945	31.828698
584.755804	38270.178104	31.833716
585.480411	38336.821194	31.838733
586.077476	38398.785594	31.843751
586.387946	38471.927502	31.848768
587.335459	38525.984091	31.853786
587.405538	38598.058337	31.858804
588.217219	38660.638363	31.863821
589.197578	38729.589045	31.868839
589.512893	38797.321105	31.873856
589.871256	38860.633387	31.878874
590.451332	38933.483162	31.883892
591.013781	38992.882676	31.888909
591.892324	39048.271686	31.893927
591.713698	39122.106341	31.898944
592.790064	39176.677008	31.903962
593.276373	39249.363625	31.908980
594.036561	39311.121040	31.913997
594.500197	39372.081741	31.919015
595.101826	39437.426543	31.924032
595.776600	39493.718703	31.929050
596.245611	39576.946526	31.934068
596.642010	39638.661063	31.939085
597.078978	39700.514305	31.944103
597.239883	39778.841112	31.949120
598.163643	39855.384737	31.954138
599.070083	39929.055731	31.959156
599.844156	39998.784005	31.964173
600.557340	40073.560859	31.969191
600.814791	40146.273104	31.974208
601.703899	40209.262305	31.979226
602.167882	40286.695100	31.984244
603.023103	40356.714360	31.989261
603.787901	40419.080851	31.994279
604.177006	40491.397010	31.999296
605.114883	40556.055624	32.004314
605.756961	40629.627946	32.009332
605.917098	40699.855062	32.014349
606.864657	40765.062109	32.019367
606.904407	40845.503366	32.024384
607.866971	40918.231424	32.029402
608.382793	40982.121617	32.034420
608.944672	41051.447008	32.039437
609.756306	41130.912575	32.044455
610.195019	41211.624053	32.049472
610.445410	41276.335796	32.054490
611.462405	41360.244995	32.059508
612.085243	41430.524609	32.064525
613.049591	41491.794634	32.069543
613.514102	41578.564951	32.074560
614.277864	41640.020192	32.079578
614.915245	41711.807543	32.084596
615.791725	41776.767882	32.089613
616.384054	41844.007527	32.094631
616.758964	41914.036385	32.099648
617.535006	41978.676238	32.104666
618.159823	42052.395984	32.109684
618.739217	42117.002554	32.114701
619.726436	42179.530769	32.119719
620.190216	42244.074824	32.124736
621.078394	42308.321570	32.129754
621.420125	42372.624218	32.134772
621.872453	42434.521950	32.139789
622.805554	42500.817264	32.144807
623.304803	42563.168613	32.149824
623.896024	42630.370243	32.154842
624.488039	42693.012930	32.159860
625.056164	42756.003921	32.164877
626.102655	42813.611784	32.169895
626.379254	42892.753498	32.174912
626.954809	42960.344097	32.179930
627.493401	43031.925563	32.184948
628.011042	43093.802050	32.189965
628.822323	43168.193129	32.194983
629.355537	43243.132525	32.200000
629.828838	43304.499243	32.205018
630.648623	43375.782918	32.210036
630.872244	43450.060803	32.215053
631.698748	43513.734640	32.220071
632.345432	43591.542502	32.225088
633.038836	43665.149927	32.230106
633.661888	43716.512674	32.235124
634.233047	43787.763275	32.240141
634.704393	43835.469891	32.245159
635.100883	43907.605510	32.250176
635.861333	43971.519169	32.255194
636.657892	44042.190365	32.260212
637.254078	44115.553574	32.265229
637.713735	44177.623214	32.270247
638.477233	44248.622721	32.275264
638.625585	44325.082569	32.280282
639.818174	44388.272550	32.285300
640.183689	44461.902617	32.290317
640.874573	44545.144403	32.295335
641.352968	44615.014698	32.300352
642.060764	44697.929133	32.305370
642.804072	44775.703818	32.310388
643.453918	44852.954337	32.315405
644.261709	44924.274302	32.320423
644.875439	44995.910829	32.325440
645.051022	45070.499884	32.330458
645.779639	45146.544987	32.335476
646.430148	45221.690754	32.340493
647.057916	45301.043451	32.345511
647.822590	45390.980518	32.350528
648.917136	45476.531065	32.355546
649.334054	45551.069459	32.360564
649.863799	45637.778329	32.365581
650.820372	45702.379071	32.370599
651.312190	45783.973025	32.375616
652.042899	45865.537283	32.380634
652.819798	45935.069408	32.385652
653.113326	46019.536030	32.390669
653.768553	46103.428465	32.395687
654.744923	46189.614406	32.400704
655.266056	46258.987934	32.405722
656.065904	46331.871343	32.410740
656.578769	46416.979228	32.415757
657.245576	46483.029509	32.420775
657.979364	46574.859404	32.425792
658.582928	46651.098613	32.430810
659.522857	46733.475152	32.435828
660.222589	46814.650720	32.440845
660.654166	46894.879404	32.445863
661.224882	46984.726649	32.450880
661.877029	47060.533138	32.455898
662.894814	47122.627485	32.460916
663.575246	47213.698746	32.465933
664.092895	47279.432250	32.470951
665.011115	47359.531854	32.475968
665.557274	47444.029329	32.480986
666.842007	47515.355941	32.486004
667.222830	47589.911468	32.491021
667.799673	47662.508435	32.496039
668.807148	47734.197543	32.501056
669.091767	47807.241323	32.506074
670.162299	47877.215166	32.511092
670.621249	47949.794832	32.516109
671.289428	48021.702216	32.521127
671.739544	48095.183961	32.526144
672.198194	48164.704253	32.531162
673.118011	48240.215337	32.536180
673.596803	48317.486148	32.541197
674.579312	48390.877794	32.546215
674.909571	48473.874341	32.551232
675.627047	48553.566858	32.556250
676.149976	48622.250724	32.561268
676.602508	48714.668030	32.566285
677.763221	48782.883761	32.571303
678.392043	48851.393016	32.576320
679.034659	48924.621858	32.581338
679.639687	48987.403261	32.586356
679.656780	49066.534744	32.591373
681.013764	49135.031931	32.596391
681.664076	49206.062387	32.601408
682.209143	49275.496608	32.606426
682.734211	49348.497002	32.611444
683.014190	49431.016458	32.616461
683.730524	49507.374734	32.621479
684.461196	49590.511996	32.626496
685.388903	49684.279784	32.631514
685.711131	49756.108770	32.636532
686.231293	49845.368220	32.641549
686.955768	49928.466905	32.646567
687.937681	50013.617416	32.651584
688.362724	50105.313181	32.656602
689.390466	50187.004667	32.661620
690.180007	50278.975757	32.666637
691.001555	50364.726034	32.671655
692.112724	50445.406721	32.676672
692.153809	50520.857352	32.681690
693.147822	50602.935201	32.686708
694.111995	50693.407486	32.691725
695.058450	50771.987912	32.696743
695.507810	50840.000120	32.701760
695.868052	50925.677584	32.706778
696.654433	51009.838282	32.711796
697.593141	51087.530538	32.716813
698.820207	51157.923159	32.721831
699.637774	51230.721183	32.726848
700.213666	51316.636342	32.731866
700.834731	51378.784816	32.736884
701.516429	51459.231223	32.741901
702.033672	51542.750160	32.746919
702.791526	51611.737458	32.751936
703.476942	51695.690403	32.756954
704.092539	51770.147447	32.761972
704.739060	51855.396281	32.766989
705.225688	51939.844342	32.772007
706.236604	52010.048378	32.777024
706.749970	52091.940380	32.782042
707.459353	52179.479835	32.787060
708.066292	52266.758653	32.792077
708.841989	52352.790633	32.797095
709.623579	52442.069314	32.802112
710.107242	52525.749640	32.807130
711.159490	52605.116006	32.812148
711.754274	52683.932911	32.817165
712.452839	52771.085103	32.822183
713.230842	52857.820201	32.827200
713.745851	52949.110143	32.832218
714.572660	53021.957552	32.837236
715.211290	53112.185352	32.842253
715.928915	53197.706267	32.847271
716.701678	53276.395026	32.852288
717.389537	53365.390161	32.857306
718.366502	53448.721150	32.862324
718.828393	53539.972083	32.867341
719.555461	53619.377398	32.872359
720.175887	53705.352550	32.877376
720.633437	53803.188891	32.882394
721.629324	53889.109055	32.887412
722.379437	53968.208694	32.892429
722.711167	54055.073450	32.897447
723.943736	54147.210625	32.902464
724.490773	54240.156646	32.907482
725.545944	54319.725332	32.912500
726.129120	54397.799154	32.917517
726.472702	54483.855091	32.922535
727.631644	54560.437956	32.927552
727.936561	54636.859110	32.932570
728.951629	54709.163518	32.937588
729.488511	54804.230547	32.942605
729.914759	54883.077824	32.947623
730.889516	54971.956934	32.952640
731.144570	55053.474347	32.957658
732.151749	55138.083827	32.962676
732.750443	55235.284693	32.967693
733.485414	55318.031755	32.972711
734.392573	55413.274244	32.977728
735.294573	55495.842771	32.982746
735.686145	55587.696113	32.987764
736.297927	55680.783518	32.992781
737.384052	55775.075603	32.997799
738.314994	55866.190177	33.002816
738.611415	55957.921955	33.007834
739.633228	56050.703151	33.012852
740.264720	56140.377266	33.017869
740.817079	56236.882981	33.022887
741.796267	56327.802121	33.027904
742.478458	56428.122885	33.032922
743.232393	56514.239803	33.037940
743.889435	56608.309822	33.042957
744.765615	56713.907920	33.047975
745.998975	56792.458644	33.052992
746.535891	56894.297087	33.058010
747.627245	56977.251180	33.063028
748.324604	57068.883828	33.068045
748.984706	57172.927663	33.073063
749.777459	57243.363351	33.078080
750.346370	57349.281041	33.083098
751.474818	57432.932328	33.088116
751.824763	57526.419216	33.093133
752.639187	57616.259275	33.098151
753.658752	57701.534809	33.103168
753.892163	57806.619378	33.108186
754.989094	57896.578266	33.113204
756.102588	57993.328244	33.118221
756.498867	58083.422825	33.123239
757.524505	58171.069162	33.128256
757.988067	58253.569949	33.133274
759.090738	58348.490758	33.138292
759.704833	58433.735359	33.143309
760.227668	58536.481846	33.148327
761.013382	58625.199949	33.153344
761.629835	58719.217064	33.158362
762.280191	58808.963197	33.163380
763.659448	58905.338653	33.168397
764.201408	59008.122296	33.173415
765.322432	59100.932806	33.178432
765.573381	59198.539068	33.183450
766.641665	59286.695110	33.188468
767.277385	59374.784050	33.193485
767.886519	59483.133147	33.198503
768.807231	59560.393950	33.203520
769.379021	59659.339753	33.208538
770.199008	59755.950816	33.213556
771.302095	59853.096956	33.218573
771.889859	59952.041544	33.223591
772.625892	60040.995276	33.228608
773.317897	60138.033815	33.233626
773.764056	60229.197808	33.238644
774.862349	60324.836479	33.243661
775.302659	60425.349888	33.248679
776.612004	60517.933490	33.253696
777.217153	60611.714763	33.258714
777.719316	60691.412890	33.263732
778.623989	60782.490876	33.268749
779.033682	60870.939707	33.273767
780.039116	60954.821863	33.278784
780.537733	61047.914880	33.283802
781.528147	61140.952255	33.288820
782.344228	61242.621061	33.293837
782.571324	61344.697501	33.298855
783.753670	61427.623223	33.303872
784.487788	61534.944959	33.308890
785.157651	61636.298597	33.313908
785.818344	61728.160666	33.318925
786.323172	61836.545850	33.323943
787.337049	61932.218659	33.328960
788.391539	62045.829733	33.333978
789.221507	62142.374600	33.338996
790.095797	62247.388766	33.344013
790.835386	62349.834213	33.349031
791.817183	62441.128053	33.354048
792.657244	62547.400942	33.359066
793.183512	62650.894514	33.364084
794.354403	62758.826740	33.369101
795.283705	62850.548263	33.374119
796.449613	62943.463654	33.379136
797.040516	63038.927134	33.384154
797.642905	63140.381521	33.389172
798.447125	63229.792949	33.394189
799.362083	63338.958911	33.399207
800.105035	63427.085498	33.404224
801.276302	63529.560224	33.409242
801.860079	63619.667204	33.414260
802.746339	63715.628581	33.419277
803.386848	63822.326637	33.424295
804.106024	63917.507462	33.429312
805.045412	64013.423503	33.434330
805.422663	64117.334667	33.439348
806.552679	64214.598164	33.444365
807.259706	64318.594859	33.449383
808.124731	64415.694523	33.454400
809.002812	64529.550732	33.459418
809.599229	64636.443589	33.464436
810.204090	64728.783394	33.469453
811.029450	64843.705740	33.474471
811.927910	64952.187548	33.479488
812.726944	65068.556818	33.484506
813.675500	65177.581496	33.489524
814.650819	65281.475408	33.494541
815.055159	65393.575078	33.499559
816.183989	65495.946412	33.504576
817.044450	65602.282159	33.509594
818.167700	65714.732456	33.514612
818.815232	65812.816556	33.519629
819.634828	65923.244624	33.524647
819.969917	66022.196908	33.529664
821.239176	66125.129714	33.534682
821.813410	66234.942522	33.539700
822.517458	66345.006281	33.544717
823.546501	66460.207280	33.549735
824.734781	66562.333757	33.554752
825.618024	66664.188755	33.559770
826.001575	66770.817938	33.564788
826.749547	66866.279295	33.569805
827.693424	66972.431169	33.574823
828.663955	67089.004568	33.579840
829.665556	67185.753098	33.584858
830.294103	67301.461182	33.589876
831.157585	67389.078770	33.594893
831.893304	67490.804106	33.599911
832.744353	67589.741643	33.604928
833.734598	67680.020173	33.609946
834.264661	67775.426849	33.614964
835.330892	67869.815868	33.619981
836.050085	67971.293350	33.624999
836.877198	68064.224349	33.630016
837.547378	68167.380029	33.635034
838.211599	68276.682775	33.640052
839.660649	68370.251996	33.645069
840.196962	68475.612627	33.650087
840.749300	68574.484039	33.655104
841.739067	68684.955324	33.660122
842.237253	68792.005676	33.665140
843.357103	68893.541434	33.670157
843.932600	69008.945149	33.675175
844.859690	69111.525481	33.680192
845.509774	69228.195266	33.685210
846.564007	69348.415560	33.690228
847.700475	69460.719226	33.695245
848.413715	69575.793401	33.700263
848.862095	69681.895362	33.705280
850.096573	69790.928195	33.710298
850.557950	69903.307904	33.715316
851.755034	70028.472029	33.720333
852.560034	70142.857503	33.725351
853.518161	70257.951753	33.730368
854.684036	70368.731434	33.735386
855.662139	70489.640997	33.740404
856.519418	70589.919330	33.745421
857.208777	70703.416365	33.750439
857.653053	70814.817236	33.755456
859.160697	70925.182832	33.760474
859.673831	71051.667489	33.765492
860.699804	71154.911540	33.770509
861.543194	71271.788119	33.775527
862.529329	71382.678635	33.780544
863.157482	71496.955121	33.785562
863.607576	71620.405582	33.790580
864.590364	71737.830754	33.795597
865.678703	71860.190538	33.800615
866.436497	71974.808558	33.805632
867.407794	72092.522123	33.810650
868.151734	72214.118783	33.815668
869.251060	72340.868166	33.820685
870.142014	72456.358367	33.825703
871.291912	72568.296607	33.830720
872.450554	72675.813567	33.835738
872.969518	72796.103704	33.840756
874.040763	72901.897154	33.845773
874.666866	73012.621574	33.850791
875.570630	73135.120262	33.855808
876.652289	73242.633786	33.860826
877.634940	73363.040089	33.865844
878.499633	73472.551103	33.870861
879.423128	73586.587371	33.875879
880.523950	73694.681779	33.880896
880.970482	73812.074044	33.885914
881.915938	73922.434053	33.890932
883.133596	74030.662582	33.895949
883.800507	74142.214465	33.900967
884.436572	74264.276786	33.905984
885.528118	74379.908435	33.911002
885.966659	74495.566473	33.916020
887.124485	74606.811850	33.921037
888.118690	74725.124017	33.926055
888.873764	74844.197366	33.931072
889.820379	74945.423386	33.936090
890.459230	75055.049231	33.941108
891.475125	75159.528269	33.946125
892.728522	75267.023331	33.951143
893.282763	75371.168619	33.956160
894.196286	75473.680127	33.961178
895.211028	75584.511383	33.966196
896.062601	75687.761476	33.971213
896.817541	75795.075909	33.976231
897.513808	75898.232499	33.981248
898.360243	76005.039482	33.986266
898.898834	76123.870921	33.991284
900.174612	76240.430604	33.996301
900.978749	76352.673051	34.001319
901.572325	76474.539584	34.006336
902.405698	76591.313427	34.011354
903.455990	76721.068998	34.016372
904.380776	76851.978276	34.021389
905.423696	76967.353219	34.026407
906.078029	77091.060024	34.031424
907.098092	77209.020670	34.036442
907.751415	77350.863461	34.041460
908.664085	77469.469445	34.046477
909.805980	77598.297814	34.051495
910.177097	77735.584888	34.056512
911.146797	77855.182896	34.061530
912.230930	77993.960288	34.066548
913.229631	78136.332884	34.071565
914.340548	78271.989115	34.076583
915.156503	78397.143938	34.081600
916.231185	78523.028393	34.086618
916.867428	78660.270959	34.091636
918.024849	78790.362416	34.096653
918.957321	78920.346337	34.101671
919.962937	79067.221259	34.106688
921.308999	79195.164742	34.111706
921.839005	79321.042528	34.116724
922.961009	79459.557029	34.121741
924.380596	79580.038699	34.126759
924.965508	79722.635263	34.131776
925.708646	79840.358224	34.136794
926.592855	79973.550799	34.141812
927.850950	80101.779660	34.146829
928.643740	80229.276462	34.151847
929.617885	80368.535827	34.156864
931.080809	80486.143111	34.161882
931.818776	80615.675513	34.166900
932.848125	80735.222008	34.171917
933.889652	80862.864694	34.176935
935.003706	80985.017556	34.181952
936.028197	81100.492660	34.186970
936.649390	81229.883385	34.191988
937.626615	81354.933015	34.197005
938.574538	81474.920727	34.202023
939.463864	81609.697318	34.207040
940.249209	81727.239603	34.212058
941.137407	81857.165436	34.217076
942.078216	81984.679220	34.222093
943.070517	82110.673147	34.227111
943.652938	82248.262639	34.232128
944.855341	82356.692129	34.237146
945.554563	82502.216423	34.242164
946.580910	82631.826446	34.247181
947.563268	82747.512962	34.252199
947.991531	82898.443331	34.257216
949.068596	83031.735742	34.262234
950.021495	83170.193202	34.267252
950.779146	83296.827160	34.272269
952.129416	83439.731608	34.277287
952.839569	83564.179439	34.282304
953.998162	83694.273401	34.287322
954.712415	83815.969659	34.292340
955.411241	83938.112004	34.297357
956.803300	84062.266264	34.302375
957.403534	84202.781268	34.307392
958.599538	84325.159794	34.312410
959.423728	84460.659831	34.317428
960.365765	84586.245341	34.322445
961.504518	84719.062729	34.327463
962.198129	84850.840877	34.332480
963.255684	84976.719432	34.337498
963.768138	85120.690254	34.342516
964.735656	85264.966359	34.347533
966.487135	85401.115785	34.352551
967.224760	85538.414427	34.357568
968.260521	85664.167417	34.362586
969.511236	85802.977307	34.367604
970.284055	85954.174276	34.372621
971.398711	86080.391027	34.377639
971.900144	86209.671225	34.382656
973.292181	86349.802456	34.387674
974.090860	86487.431930	34.392692
974.814088	86633.610898	34.397709
975.986254	86772.825511	34.402727
976.563904	86924.105288	34.407744
977.764734	87058.324147	34.412762
978.782565	87200.528276	34.417780
979.925949	87345.306980	34.422797
981.125897	87500.309657	34.427815
981.683316	87644.902330	34.432832
983.108022	87777.696079	34.437850
984.271113	87914.558539	34.442868
984.705342	88065.451674	34.447885
986.021270	88205.669795	34.452903
986.976356	88351.517288	34.457920
987.847213	88496.512625	34.462938
989.211929	88643.933207	34.467956
989.872316	88786.471746	34.472973
990.998513	88923.491670	34.477991
991.897401	89078.503804	34.483008
993.131990	89221.911921	34.488026
994.098633	89360.985860	34.493044
994.895660	89515.005103	34.498061
996.567780	89654.331148	34.503079
997.410142	89808.097964	34.508096
997.859607	89937.255170	34.513114
999.300577	90084.615074	34.518132
1000.302998	90234.668508	34.523149
1001.745606	90368.752139	34.528167
1002.439030	90511.371424	34.533184
1003.270559	90648.076535	34.538202
1004.555755	90788.738921	34.543220
1004.961630	90942.509215	34.548237
1006.777386	91081.338786	34.553255
1007.566963	91222.288179	34.558272
1008.513861	91360.940247	34.563290
1009.597878	91507.215985	34.568308
1010.507757	91650.160630	34.573325
1011.768962	91786.756827	34.578343
1012.395919	91937.832302	34.583360
1013.518058	92078.529148	34.588378
1014.650530	92214.731309	34.593396
1015.638382	92365.439630	34.598413
1016.495805	92498.878643	34.603431
1017.534068	92641.649654	34.608448
1018.299474	92785.859094	34.613466
1019.481459	92933.810843	34.618484
1020.230746	93076.309375	34.623501
1020.990521	93203.483186	34.628519
1021.922903	93346.611289	34.633536
1022.925606	93487.886683	34.638554
1024.005276	93631.441498	34.643572
1024.555050	93782.262635	34.648589
1025.655567	93924.651054	34.653607
1026.682537	94068.185486	34.658624
1027.703002	94223.109140	34.663642
1028.857160	94375.872177	34.668660
1029.656212	94538.746727	34.673677
1030.798620	94693.210079	34.678695
1031.722038	94837.259844	34.683712
1032.542572	94998.336162	34.688730
1033.940581	95149.671063	34.693748
1034.347692	95322.566402	34.698765
1035.497994	95478.122121	34.703783
1036.773818	95651.369858	34.708800
1037.784871	95816.407989	34.713818
1038.698477	95986.863031	34.718836
1039.466548	96150.310347	34.723853
1040.917960	96321.356093	34.728871
1041.760186	96490.402054	34.733888
1042.728094	96666.068989	34.738906
1043.883086	96837.882621	34.743924
1044.659913	97022.123449	34.748941
1046.138620	97193.689751	34.753959
1047.107642	97360.732824	34.758976
1048.191839	97535.323080	34.763994
1049.223500	97710.657594	34.769012
1050.528304	97886.068450	34.774029
1051.661663	98061.306289	34.779047
1052.050865	98235.908689	34.784064
1053.509206	98420.230657	34.789082
1054.729921	98606.283611	34.794100
1055.698993	98780.559646	34.799117
1056.633865	98955.874486	34.804135
1057.743325	99131.611174	34.809152
1058.867084	99315.944328	34.814170
1060.038141	99490.729981	34.819188
1061.005388	99666.139331	34.824205
1062.202240	99848.887794	34.829223
1063.557223	100031.972303	34.834240
1064.258853	100201.129638	34.839258
1065.852914	100375.218278	34.844276
1066.780262	100553.286818	34.849293
1067.807735	100720.563935	34.854311
1068.974301	100907.155480	34.859328
1069.694859	101077.043582	34.864346
1071.176316	101252.600380	34.869364
1071.784723	101443.099698	34.874381
1073.135748	101620.358445	34.879399
1074.142252	101802.702741	34.884416
1075.431734	101988.901891	34.889434
1076.548304	102155.445438	34.894452
1077.407066	102345.416130	34.899469
1078.480349	102512.488337	34.904487
1079.741953	102694.442146	34.909504
1080.748856	102873.684937	34.914522
1081.764800	103051.838361	34.919540
1082.672619	103244.485946	34.924557
1084.096895	103412.101109	34.929575
1085.295824	103585.086262	34.934592
1086.355638	103768.239708	34.939610
1087.248775	103948.509170	34.944628
1088.282883	104128.984526	34.949645
1089.581715	104305.617969	34.954663
1090.586820	104479.021006	34.959680
1091.696769	104641.085538	34.964698
1092.976751	104801.223228	34.969716
1093.590862	104975.365415	34.974733
1094.600838	105128.508029	34.979751
1095.918717	105296.912715	34.984768
1096.890763	105476.331028	34.989786
1098.079817	105636.184849	34.994804
1098.946040	105814.647724	34.999821
1100.046402	105978.811825	35.004839
1100.988123	106156.466592	35.009856
1101.836033	106339.026973	35.014874
1103.429451	106521.275362	35.019892
1104.273916	106696.315350	35.024909
1105.323541	106876.338238	35.029927
1106.362433	107062.279103	35.034944
1107.318665	107256.695826	35.039962
1108.516484	107431.808866	35.044980
1109.608660	107641.151908	35.049997
1110.907436	107819.278007	35.055015
1112.179960	108006.858741	35.060032
1112.995184	108202.686256	35.065050
1114.186004	108392.005818	35.070068
1115.030638	108585.829935	35.075085
1116.031348	108784.379663	35.080103
1116.999557	108984.025567	35.085120
1117.897124	109186.610681	35.090138
1119.676535	109385.099401	35.095156
1120.862700	109589.020507	35.100173
1121.848609	109796.092381	35.105191
1123.435807	109991.779851	35.110208
1124.408176	110183.833491	35.115226
1125.643259	110386.257717	35.120244
1126.652661	110591.900314	35.125261
1127.808318	110786.904763	35.130279
1129.116680	110985.989707	35.135296
1130.216793	111182.260255	35.140314
1131.116376	111382.239058	35.145332
1132.088212	111590.593606	35.150349
1133.522746	111787.611263	35.155367
1134.540952	111990.273171	35.160384
1135.771459	112202.250681	35.165402
1137.147215	112406.579415	35.170420
1138.048647	112617.068953	35.175437
1139.065266	112808.297439	35.180455
1140.213183	113022.727235	35.185472
1141.257441	113234.236658	35.190490
1142.654345	113433.653946	35.195508
1143.517055	113641.294450	35.200525
1144.902941	113849.572137	35.205543
1146.300114	114053.934736	35.210560
1147.209367	114278.675633	35.215578
1148.652436	114468.844096	35.220596
1149.798852	114677.154839	35.225613
1150.552087	114889.206286	35.230631
1152.083717	115093.123436	35.235648
1152.948572	115302.980357	35.240666
1154.157783	115504.913951	35.245684
1155.294674	115715.679190	35.250701
1156.614934	115929.785897	35.255719
1157.742807	116124.781517	35.260736
1158.540862	116344.539840	35.265754
1160.116226	116545.343322	35.270772
1161.087587	116762.187387	35.275789
1162.061981	116964.892358	35.280807
1163.390812	117177.828654	35.285824
1164.270580	117399.000663	35.290842
1165.580993	117604.948973	35.295860
1167.085008	117813.286878	35.300877
1167.823686	118011.007873	35.305895
1168.867407	118218.018322	35.310912
1170.201376	118411.462213	35.315930
1171.331565	118618.524588	35.320948
1172.919293	118821.115872	35.325965
1173.453412	119021.538546	35.330983
1174.875537	119227.289864	35.336000
1175.862091	119432.671137	35.341018
1177.295063	119630.212351	35.346036
1178.162603	119834.234917	35.351053
1179.104427	120046.559326	35.356071
1180.652273	120254.058472	35.361088
1181.703777	120476.239265	35.366106
1182.764990	120682.516670	35.371124
1183.742200	120895.956509	35.376141
1185.068045	121117.894035	35.381159
1186.543534	121333.459640	35.386176
1187.509789	121554.382737	35.391194
1188.832146	121772.663414	35.396212
1189.922317	121988.867749	35.401229
1191.131072	122212.999854	35.406247
1192.414872	122430.404643	35.411264
1193.347960	122661.492380	35.416282
1194.859908	122879.280930	35.421300
1195.960476	123111.523047	35.426317
1197.048820	123334.112000	35.431335
1198.569233	123562.904462	35.436352
1199.761461	123794.921266	35.441370
1201.015858	124011.379203	35.446388
1202.427205	124236.354741	35.451405
1203.256164	124472.568393	35.456423
1204.700762	124695.463365	35.461440
1206.001775	124921.666242	35.466458
1206.925180	125147.806485	35.471476
1208.530041	125375.052467	35.476493
1209.430366	125605.027484	35.481511
1211.225979	125835.071697	35.486528
1212.003837	126068.479816	35.491546
1213.322255	126292.826849	35.496564
1214.943122	126520.420904	35.501581
1215.983312	126745.032698	35.506599
1217.502998	126965.346186	35.511616
1218.398440	127194.294582	35.516634
1219.722305	127412.324137	35.521652
1220.728170	127639.521111	35.526669
1222.096057	127880.919377	35.531687
1223.814700	128099.547609	35.536704
1225.042792	128325.736876	35.541722
1226.464617	128549.728271	35.546740
1227.597569	128768.458009	35.551757
1228.358571	129001.282583	35.556775
1230.066210	129207.777224	35.561792
1231.268791	129437.198348	35.566810
1232.399923	129660.028859	35.571828
1233.594052	129875.536538	35.576845
1234.583844	130098.963927	35.581863
1235.960621	130317.372581	35.586880
1237.225389	130549.516863	35.591898
1238.599935	130785.561661	35.596916
1239.716950	131006.172957	35.601933
1240.999078	131229.255746	35.606951
1242.312022	131452.094146	35.611968
1243.559161	131680.750866	35.616986
1244.811739	131896.604851	35.622004
1246.156838	132118.010103	35.627021
1247.168709	132352.541823	35.632039
1248.479333	132570.304947	35.637056
1249.599304	132794.186039	35.642074
1250.814923	133016.151302	35.647092
1252.135345	133220.644226	35.652109
1253.416364	133433.524651	35.657127
1254.616807	133637.963974	35.662144
1255.947238	133849.596573	35.667162
1257.031449	134058.177924	35.672180
1258.343675	134269.309154	35.677197
1259.394591	134497.916795	35.682215
1259.903473	134708.118714	35.687232
1261.717585	134947.049841	35.692250
1262.594767	135169.554778	35.697268
1264.140525	135394.397572	35.702285
1265.468035	135618.301757	35.707303
1266.557639	135843.083545	35.712320
1267.804477	136078.300484	35.717338
1269.343717	136309.806697	35.722356
1270.265053	136543.217003	35.727373
1271.602162	136781.504870	35.732391
1273.038661	137021.109272	35.737408
1274.009956	137254.021821	35.742426
1274.947793	137503.614219	35.747444
1276.500097	137747.540844	35.752461
1277.429452	137993.981223	35.757479
1279.147173	138237.313497	35.762496
1280.234660	138490.210402	35.767514
1281.693714	138740.283685	35.772532
1283.303799	138973.584338	35.777549
1284.370181	139240.348924	35.782567
1285.673902	139482.097540	35.787584
1287.454538	139716.947366	35.792602
1288.384804	139974.534730	35.797620
1289.931526	140208.171289	35.802637
1291.222896	140467.947008	35.807655
1292.726266	140702.950851	35.812672
1294.037124	140951.999672	35.817690
1295.677960	141199.258555	35.822708
1297.004436	141438.544517	35.827725
1298.149788	141675.896601	35.832743
1299.339910	141918.391185	35.837760
1300.682391	142167.430818	35.842778
1302.048794	142409.734832	35.847796
1303.508230	142647.548838	35.852813
1304.576237	142901.077322	35.857831
1306.032946	143145.552598	35.862848
1307.088418	143390.539725	35.867866
1308.518951	143641.604221	35.872884
1310.212315	143882.329916	35.877901
1311.357921	144140.191441	35.882919
1312.399361	144380.381518	35.887936
1314.057191	144627.116427	35.892954
1315.191174	144877.883588	35.897972
1316.275697	145132.401768	35.902989
1317.510780	145382.268034	35.908007
1319.186208	145628.626482	35.913024
1320.780838	145881.746748	35.918042
1322.062530	146135.351699	35.923060
1323.729998	146365.559628	35.928077
1324.598492	146627.061160	35.933095
1326.126776	146863.052956	35.938112
1327.625186	147102.297898	35.943130
1328.771276	147350.480336	35.948148
1330.122836	147590.399549	35.953165
1331.475533	147831.588403	35.958183
1332.799591	148077.932740	35.963200
1334.119629	148319.092141	35.968218
1335.403072	148565.966445	35.973236
1336.925068	148807.476141	35.978253
1338.268688	149040.050005	35.983271
1339.469278	149277.240242	35.988288
1341.014736	149499.903502	35.993306
1342.077073	149734.164320	35.998324
1343.725741	149944.890930	36.003341
1344.700578	150174.108322	36.008359
1345.779419	150402.054260	36.013376
1347.625847	150636.254541	36.018394
1348.331881	150876.834363	36.023412
1349.588687	151099.833860	36.028429
1350.711033	151346.118945	36.033447
1352.069703	151594.827240	36.038464
1353.582723	151832.032679	36.043482
1354.731239	152077.379560	36.048500
1356.248522	152337.266482	36.053517
1357.295214	152588.975529	36.058535
1358.610722	152834.325027	36.063552
1360.252387	153096.454331	36.068570
1361.235065	153356.170122	36.073588
1362.673866	153611.195102	36.078605
1364.091978	153874.597026	36.083623
1365.301554	154141.028789	36.088640
1367.206112	154401.474457	36.093658
1368.360255	154663.504642	36.098676
1369.976473	154917.126196	36.103693
1371.304222	155200.137566	36.108711
1372.465612	155453.127382	36.113728
1374.059590	155710.246132	36.118746
1375.390953	155991.740354	36.123764
1377.101083	156245.849652	36.128781
1378.469395	156510.152752	36.133799
1379.730967	156771.430711	36.138816
1381.334848	157035.774470	36.143834
1382.351603	157308.526149	36.148852
1383.652706	157566.923099	36.153869
1385.186824	157835.609505	36.158887
1386.862480	158109.120348	36.163904
1388.275580	158372.920852	36.168922
1389.452688	158652.036177	36.173940
1391.003275	158906.315501	36.178957
1392.220902	159186.506114	36.183975
1393.765715	159457.979767	36.188992
1395.412968	159724.744291	36.194010
1396.566063	160004.392941	36.199028
1398.055288	160276.058784	36.204045
1399.859826	160557.062476	36.209063
1401.143936	160820.240301	36.214080
1402.401851	161077.473968	36.219098
1403.791180	161354.847090	36.224116
1405.286965	161624.363858	36.229133
1406.761151	161898.567476	36.234151
1408.334388	162163.837399	36.239168
1409.840390	162431.213503	36.244186
1411.065399	162704.689608	36.249204
1412.432231	162960.267414	36.254221
1413.928976	163235.985769	36.259239
1415.463516	163509.504700	36.264256
1416.903864	163774.743192	36.269274
1417.977308	164051.907021	36.274292
1419.673390	164314.340644	36.279309
1421.527478	164591.036359	36.284327
1422.675555	164847.613138	36.289344
1424.059604	165113.300543	36.294362
1425.412289	165387.203991	36.299380
1427.120914	165646.002083	36.304397
1428.288209	165919.330462	36.309415
1429.500432	166187.450873	36.314432
1430.791249	166446.601867	36.319450
1432.200456	166729.982626	36.324468
1433.454617	166979.930912	36.329485
1435.871682	167236.045467	36.334503
1436.774892	167488.186301	36.339520
1438.190002	167731.666312	36.344538
1439.226635	167990.982497	36.349556
1440.821205	168246.096748	36.354573
1442.048265	168502.313676	36.359591
1443.461130	168767.612141	36.364608
1444.781982	169025.643763	36.369626
1446.139661	169303.377202	36.374644
1447.586290	169568.611311	36.379661
1449.052599	169846.558507	36.384679
1450.154399	170127.384689	36.389696
1451.702621	170395.715716	36.394714
1452.828023	170674.193754	36.399732
1454.860468	170957.294915	36.404749
1456.166272	171235.429265	36.409767
1457.354694	171526.058822	36.414784
1458.854826	171802.578199	36.419802
1460.031999	172102.324577	36.424820
1461.451507	172394.545646	36.429837
1463.041083	172683.174473	36.434855
1464.467062	172980.639139	36.439872
1466.029351	173277.842022	36.444890
1467.341637	173578.869813	36.449908
1469.044718	173878.845059	36.454925
1470.604136	174177.094612	36.459943
1471.928664	174482.364689	36.464960
1473.697304	174769.364770	36.469978
1475.073212	175081.318146	36.474996
1476.613093	175379.946351	36.480013
1478.011180	175683.396997	36.485031
1479.447540	175984.508036	36.490048
1481.491469	176284.149874	36.495066
1482.730730	176594.536344	36.500084
1483.946098	176895.727512	36.505101
1486.106963	177193.870631	36.510119
1487.330833	177505.635978	36.515136
1489.195323	177797.612849	36.520154
1490.566149	178099.432820	36.525172
1492.103355	178402.267813	36.530189
1493.655303	178695.722974	36.535207
1495.102669	179001.254331	36.540224
1496.910062	179298.732126	36.545242
1498.427860	179607.542655	36.550260
1500.051710	179903.911995	36.555277
1501.664626	180203.762478	36.560295
1502.695967	180500.981964	36.565312
1504.492871	180787.300917	36.570330
1506.068353	181093.496130	36.575348
1507.534630	181392.692270	36.580365
1509.570926	181686.566620	36.585383
1510.831068	181985.508245	36.590400
1512.667991	182281.665410	36.595418
1514.166086	182574.034320	36.600436
1515.602495	182862.366026	36.605453
1517.367988	183154.833533	36.610471
1518.909609	183452.277146	36.615488
1520.005104	183738.651686	36.620506
1521.859688	184023.633003	36.625524
1523.027634	184325.738002	36.630541
1525.004067	184617.594626	36.635559
1526.478474	184923.676002	36.640576
1528.060498	185212.821122	36.645594
1529.266201	185503.223100	36.650612
1530.778316	185795.251494	36.655629
1532.631551	186071.599356	36.660647
1533.582587	186368.026529	36.665664
1535.108534	186641.016694	36.670682
1536.764115	186919.749686	36.675700
1538.122047	187195.892924	36.680717
1539.606513	187465.453893	36.685735
1540.969404	187741.890903	36.690752
1542.492805	188024.611600	36.695770
1544.008187	188309.746864	36.700788
1545.199706	188599.595755	36.705805
1547.193670	188884.794398	36.710823
1548.151730	189175.966828	36.715840
1549.725368	189470.022137	36.720858
1551.448777	189766.999244	36.725876
1552.449222	190070.114420	36.730893
1554.255034	190362.307805	36.735911
1555.754414	190677.149450	36.740928
1557.196359	190979.739286	36.745946
1558.447837	191283.885464	36.750964
1559.790113	191602.858257	36.755981
1561.690395	191925.625122	36.760999
1563.371006	192247.097027	36.766016
1565.157701	192565.925243	36.771034
1566.641301	192889.819689	36.776052
1567.789993	193207.906057	36.781069
1569.672931	193524.933297	36.786087
1571.009102	193861.729962	36.791104
1572.668346	194184.129449	36.796122
1574.235162	194510.646423	36.801140
1576.059966	194850.541432	36.806157
1577.884561	195167.281842	36.811175
1579.149898	195501.686752	36.816192
1581.195009	195831.394161	36.821210
1582.724385	196143.820862	36.826228
1583.876942	196481.854995	36.831245
1585.991314	196813.434875	36.836263
1587.123247	197144.632815	36.841280
1589.149679	197481.689763	36.846298
1590.696830	197809.940449	36.851316
1592.406924	198132.338363	36.856333
1594.163395	198458.450095	36.861351
1595.707665	198797.358040	36.866368
1597.608912	199131.066741	36.871386
1599.348714	199457.059037	36.876404
1600.885390	199787.733274	36.881421
1602.620994	200105.959190	36.886439
1604.209065	200440.500423	36.891456
1605.932137	200767.428458	36.896474
1607.667923	201086.344399	36.901492
1608.979320	201423.741932	36.906509
1610.790943	201744.882893	36.911527
1612.317999	202069.779739	36.916544
1613.609811	202399.389317	36.921562
1615.533171	202725.175886	36.926580
1616.978929	203059.600503	36.931597
1618.661913	203385.124993	36.936615
1620.143840	203728.421820	36.941632
1621.690726	204060.942405	36.946650
1623.651238	204395.973644	36.951668
1624.743357	204732.127519	36.956685
1626.576806	205062.535546	36.961703
1627.892142	205397.715891	36.966720
1629.751891	205740.286482	36.971738
1631.390508	206079.708082	36.976756
1632.785038	206426.802645	36.981773
1634.862208	206759.666364	36.986791
1636.462645	207094.489485	36.991808
1637.717433	207437.015073	36.996826
1639.782131	207776.792616	37.001844
1641.476596	208111.287026	37.006861
1643.320996	208424.743267	37.011879
1644.279567	208745.127681	37.016896
1646.209287	209053.531214	37.021914
1647.878193	209368.416822	37.026932
1649.015993	209691.365674	37.031949
1650.779849	210017.158285	37.036967
1652.336136	210341.462683	37.041984
1653.711590	210678.775650	37.047002
1655.601892	210999.395726	37.052020
1656.990829	211336.632870	37.057037
1658.835357	211670.316748	37.062055
1660.546978	212014.639633	37.067072
1662.039509	212344.346179	37.072090
1663.872355	212680.042168	37.077108
1664.868474	213026.442746	37.082125
1666.838313	213378.880668	37.087143
1668.156918	213731.427546	37.092160
1670.109828	214077.750287	37.097178
1671.401203	214440.412468	37.102196
1673.110346	214809.026233	37.107213
1675.023249	215162.394713	37.112231
1676.857152	215520.399927	37.117248
1678.161900	215892.005457	37.122266
1679.805109	216257.130886	37.127284
1681.430162	216622.159105	37.132301
1683.025789	216998.673424	37.137319
1684.921552	217368.053551	37.142336
1686.445815	217752.049557	37.147354
1688.540794	218125.082315	37.152372
1689.681603	218505.258611	37.157389
1691.695101	218877.698036	37.162407
1693.608119	219266.258066	37.167424
1695.131284	219649.626435	37.172442
1697.143100	220024.025941	37.177460
1698.709602	220407.694692	37.182477
1700.664457	220776.518518	37.187495
1702.238463	221162.855605	37.192512
1703.816865	221547.694788	37.197530
1705.723315	221933.573286	37.202548
1707.208787	222323.713534	37.207565
1709.440006	222699.482927	37.212583
1710.894306	223156.914001	37.217600
1712.346327	223549.222916	37.222618
1714.530241	223937.653114	37.227636
1716.337734	224329.677325	37.232653
1718.032518	224712.907726	37.237671
1719.762165	225099.359365	37.242688
1721.693174	225485.575766	37.247706
1723.486267	225858.506561	37.252724
1724.928461	226248.666877	37.257741
1726.898301	226638.715840	37.262759
1728.769003	227023.473720	37.267776
1730.459575	227407.551290	37.272794
1732.133731	227771.312400	37.277812
1733.804447	228164.869792	37.282829
1735.703534	228542.108883	37.287847
1737.403135	228933.885706	37.292864
1739.154373	229309.297089	37.297882
1741.018523	229696.349763	37.302900
1742.453092	230082.407620	37.307917
1744.260113	230470.310059	37.312935
1746.370631	230852.930811	37.317952
1747.857884	231245.993709	37.322970
1750.034842	231614.914316	37.327988
1751.842767	232014.022504	37.333005
1753.330317	232381.280758	37.338023
1755.038827	232765.522211	37.343040
1756.684882	233140.249422	37.348058
1758.808043	233495.466661	37.353076
1760.325890	233856.601580	37.358093
1762.044241	234222.555851	37.363111
1763.923420	234570.931901	37.368128
1765.597312	234936.437833	37.373146
1767.412261	235287.670925	37.378164
1768.918601	235648.811544	37.383181
1770.425129	236020.977215	37.388199
1772.518694	236398.812894	37.393216
1773.912324	236767.569491	37.398234
1776.045964	237145.450872	37.403252
1777.173638	237522.914911	37.408269
1778.769713	237906.906835	37.413287
1780.631323	238294.081703	37.418304
1782.018739	238685.476176	37.423322
1783.811203	239073.349803	37.428340
1785.595333	239479.769114	37.433357
1787.212648	239870.213346	37.438375
1788.958134	240274.557549	37.443392
1790.785912	240684.985448	37.448410
1792.809787	241089.488347	37.453428
1794.228984	241508.444177	37.458445
1795.901384	241923.345331	37.463463
1797.867152	242337.995511	37.468480
1799.460077	242763.758056	37.473498
1801.639169	243183.454882	37.478516
1803.637429	243606.992631	37.483533
1805.036745	244029.563047	37.488551
1807.329297	244449.903547	37.493568
1809.033757	244873.542532	37.498586
1811.261152	245292.421640	37.503604
1813.059548	245728.620671	37.508621
1814.584045	246142.688865	37.513639
1816.514034	246567.563032	37.518656
1818.232846	247000.220489	37.523674
1820.131042	247431.019838	37.528692
1821.881680	247865.629101	37.533709
1823.827259	248290.172485	37.538727
1825.978534	248725.250000	37.543744
1827.901796	249163.617217	37.548762
1830.124795	249584.762904	37.553780
1832.064232	250008.826360	37.558797
1833.883634	250436.745885	37.563815
1835.701511	250853.869698	37.568832
1837.413136	251279.877083	37.573850
1839.561525	251706.092092	37.578868
1841.552768	252123.010391	37.583885
1843.263927	252550.238112	37.588903
1845.032453	252963.586473	37.593920
1846.790536	253396.217839	37.598938
1848.651069	253815.927677	37.603956
1850.446512	254252.135176	37.608973
1852.521640	254674.705941	37.613991
1854.325787	255094.654284	37.619008
1856.178809	255523.155609	37.624026
1858.345567	255945.229032	37.629044
1860.108808	256366.429286	37.634061
1862.156117	256785.601265	37.639079
1864.382982	257218.182011	37.644096
1865.757523	257637.998701	37.649114
1867.524178	258060.418019	37.654132
1869.964029	258473.911234	37.659149
1871.456201	258896.706148	37.664167
1873.360694	259322.760787	37.669184
1875.207536	259746.691034	37.674202
1876.671354	260168.220362	37.679220
1879.017455	260589.959561	37.684237
1880.261477	261004.005655	37.689255
1882.381949	261411.759310	37.694272
1884.027714	261822.817459	37.699290
1885.983313	262222.748482	37.704308
1887.789136	262622.704096	37.709325
1889.128832	263031.399033	37.714343
1891.449312	263443.793108	37.719360
1892.900080	263861.970120	37.724378
1894.561860	264276.860447	37.729396
1896.384448	264710.700156	37.734413
1897.695919	265142.693347	37.739431
1899.863962	265577.847190	37.744448
1901.706738	266015.645542	37.749466
1903.492274	266459.067082	37.754484
1905.618840	266893.236006	37.759501
1907.170617	267355.773075	37.764519
1909.109215	267789.286339	37.769536
1911.017134	268243.431491	37.774554
1912.869115	268702.716792	37.779572
1914.891846	269158.264540	37.784589
1916.687547	269624.010409	37.789607
1918.865498	270085.043837	37.794624
1920.469353	270548.000473	37.799642
1922.456332	271015.008468	37.804660
1924.742816	271486.945285	37.809677
1926.428458	271964.111969	37.814695
1928.437905	272425.804992	37.819712
1930.202527	272900.670896	37.824730
1932.558203	273379.731448	37.829748
1934.541321	273858.497051	37.834765
1936.189421	274342.753257	37.839783
1938.244273	274810.810813	37.844800
1940.136105	275288.725157	37.849818
1942.532052	275770.391079	37.854836
1944.569726	276253.563117	37.859853
1945.981743	276733.052518	37.864871
1948.339524	277212.791156	37.869888
1950.461108	277694.777734	37.874906
1952.216765	278182.970956	37.879924
1954.418007	278670.098773	37.884941
1956.107076	279150.578468	37.889959
1958.335259	279646.640962	37.894976
1960.297036	280132.763245	37.899994
1962.105922	280619.976399	37.905012
1964.277063	281108.042915	37.910029
1966.303996	281594.455418	37.915047
1968.370265	282087.439099	37.920064
1970.310149	282572.694787	37.925082
1972.472453	283059.334844	37.930100
1974.486359	283552.754743	37.935117
1976.348446	284050.465636	37.940135
1978.335236	284524.455067	37.945152
1980.405047	285026.827818	37.950170
1982.441988	285513.887532	37.955188
1984.706568	285993.846624	37.960205
1986.463648	286489.712711	37.965223
1988.366839	286991.445973	37.970240
1990.497613	287479.271120	37.975258
1992.174195	287960.387613	37.980276
1994.561298	288449.640289	37.985293
1996.275936	288948.146401	37.990311
1998.353861	289439.961190	37.995328
2000.708136	289932.058722	38.000346
2002.468303	290427.960910	38.005364
2004.761403	290900.100339	38.010381
2006.379464	291397.190612	38.015399
2008.549893	291876.356999	38.020416
2010.537236	292377.039927	38.025434
2012.147946	292863.178172	38.030452
2014.475153	293335.454978	38.035469
2016.391655	293797.993512	38.040487
2018.126307	294262.236580	38.045504
2019.946743	294734.642152	38.050522
2022.276898	295210.796852	38.055540
2024.157911	295672.622432	38.060557
2025.900010	296157.048636	38.065575
2027.879948	296638.334756	38.070592
2029.732030	297114.001319	38.075610
2032.010526	297604.174113	38.080628
2034.182319	298088.571380	38.085645
2035.656037	298585.653800	38.090663
2037.593764	299060.713145	38.095680
2039.763890	299564.558692	38.100698
2041.694133	300067.755551	38.105716
2044.059191	300573.747995	38.110733
2045.867236	301093.620706	38.115751
2047.963925	301588.883525	38.120768
2049.954301	302102.701415	38.125786
2051.626032	302608.670548	38.130804
2053.886713	303131.377973	38.135821
2055.702797	303656.949484	38.140839
2058.016410	304187.235800	38.145856
2059.780121	304708.441561	38.150874
2061.767398	305242.153221	38.155892
2063.853540	305765.305807	38.160909
2065.873595	306317.265439	38.165927
2068.010459	306863.132566	38.170944
2070.420784	307404.075009	38.175962
2072.147141	307947.082341	38.180980
2074.315331	308482.292912	38.185997
2076.586019	309036.580379	38.191015
2078.715231	309579.840489	38.196032
2081.246051	310125.341553	38.201050
2083.063655	310678.803613	38.206068
2085.655017	311220.223915	38.211085
2087.615812	311776.701893	38.216103
2089.866462	312312.583982	38.221120
2091.263517	312855.383445	38.226138
2093.389063	313414.717143	38.231156
2095.950788	313969.835444	38.236173
2098.226507	314522.609781	38.241191
2100.468086	315068.376994	38.246208
2102.652858	315613.616202	38.251226
2104.807640	316173.660309	38.256244
2107.315712	316714.520901	38.261261
2109.356554	317259.136382	38.266279
2111.701411	317806.744490	38.271296
2114.113381	318344.713526	38.276314
2116.374025	318882.170071	38.281332
2118.740644	319411.276345	38.286349
2120.702259	319959.641335	38.291367
2123.178897	320481.839840	38.296384
2125.404197	321000.216240	38.301402
2127.492587	321544.916166	38.306420
2129.711320	322066.560584	38.311437
2131.801185	322599.190753	38.316455
2133.786873	323115.888537	38.321472
2136.222390	323632.964858	38.326490
2138.490926	324169.665490	38.331508
2140.602010	324685.288647	38.336525
2142.560678	325216.217120	38.341543
2144.854069	325734.314933	38.346560
2146.835915	326252.916756	38.351578
2149.192582	326777.596335	38.356596
2151.261137	327302.242704	38.361613
2153.254303	327828.470957	38.366631
2155.542820	328335.960071	38.371648
2157.694343	328823.740967	38.376666
2159.779418	329324.679572	38.381684
2161.921908	329806.614492	38.386701
2163.602324	330309.363045	38.391719
2165.805163	330797.702608	38.396736
2168.058160	331286.765884	38.401754
2169.784626	331794.266337	38.406772
2172.127203	332293.689133	38.411789
2173.710589	332807.347443	38.416807
2175.812471	333316.548981	38.421824
2178.048894	333842.681183	38.426842
2179.991761	334366.038951	38.431860
2182.391129	334888.503943	38.436877
2184.498885	335418.170509	38.441895
2186.296762	335956.843726	38.446912
2188.640987	336486.663627	38.451930
2190.382999	337032.899576	38.456948
2192.868724	337576.697083	38.461965
2194.987247	338129.966788	38.466983
2197.071531	338678.032587	38.472000
2199.522900	339223.315901	38.477018
2201.595903	339785.992223	38.482036
2203.800277	340346.356127	38.487053
2206.048973	340904.345869	38.492071
2207.974026	341461.595903	38.497088
2210.519072	342036.631326	38.502106
2212.825916	342604.465618	38.507124
2215.040186	343172.410065	38.512141
2217.255492	343741.261350	38.517159
2219.476134	344325.358621	38.522176
2221.650884	344894.507406	38.527194
2223.734757	345472.496498	38.532212
2226.013300	346042.730969	38.537229
2228.577161	346628.544933	38.542247
2230.301478	347209.084362	38.547264
2232.924908	347791.726739	38.552282
2235.263937	348390.726803	38.557300
2237.511764	348971.817242	38.562317
2239.951266	349564.592970	38.567335
2241.796219	350160.681887	38.572352
2244.524023	350750.475897	38.577370
2246.848654	351339.821050	38.582388
2249.090127	351922.498084	38.587405
2251.246012	352510.510389	38.592423
2253.842615	353106.257627	38.597440
2255.994056	353680.501234	38.602458
2258.223968	354286.417308	38.607476
2260.802025	354873.515588	38.612493
2263.121844	355470.645726	38.617511
2265.246145	356052.600794	38.622528
2267.712536	356640.454033	38.627546
2270.190329	357238.014927	38.632564
2272.308248	357821.722363	38.637581
2274.657446	358416.344143	38.642599
2276.820801	359011.267018	38.647616
2279.279530	359590.097603	38.652634
2281.530969	360178.519018	38.657652
2283.936938	360765.054219	38.662669
2286.246996	361345.380862	38.667687
2288.191238	361936.313318	38.672704
2290.802111	362532.733579	38.677722
2292.727519	363126.188206	38.682740
2295.035437	363711.757040	38.687757
2298.138649	364305.049991	38.692775
2300.018020	364896.937596	38.697792
2302.529099	365478.082716	38.702810
2304.582375	366065.560253	38.707828
2306.286730	366650.346635	38.712845
2309.007778	367206.241200	38.717863
2310.976642	367770.876159	38.722880
2313.602297	368331.386371	38.727898
2315.620443	368902.717939	38.732916
2317.908426	369464.966179	38.737933
2319.938789	370033.006091	38.742951
2321.981513	370606.057242	38.747968
2324.515041	371179.982175	38.752986
2326.108923	371776.626507	38.758004
2328.514581	372358.162798	38.763021
2330.942533	372948.359953	38.768039
2333.204226	373544.433410	38.773056
2335.323409	374141.686984	38.778074
2337.645908	374757.993915	38.783092
2339.860663	375372.862212	38.788109
2342.044312	375979.355861	38.793127
2344.189492	376593.072825	38.798144
2346.569170	377213.232188	38.803162
2349.073090	377847.408720	38.808180
2351.129385	378481.114801	38.813197
2353.585791	379113.804764	38.818215
2355.661046	379753.265523	38.823232
2358.333501	380398.041960	38.828250
2360.564917	381044.957967	38.833268
2363.011869	381694.006425	38.838285
2365.598578	382343.374042	38.843303
2367.749767	382999.671926	38.848320
2370.225799	383650.958878	38.853338
2372.632270	384311.447789	38.858356
2375.007288	384976.137087	38.863373
2377.405637	385635.307192	38.868391
2379.947732	386301.310521	38.873408
2382.518899	386956.343063	38.878426
2384.557576	387639.361862	38.883444
2387.290369	388298.320065	38.888461
2389.653099	388965.995299	38.893479
2392.057134	389644.930079	38.898496
2394.746553	390315.462995	38.903514
2397.469666	390981.945329	38.908532
2399.871611	391652.927462	38.913549
2402.625058	392314.863797	38.918567
2405.203066	392987.511109	38.923584
2407.598007	393651.023585	38.928602
2409.964221	394316.376416	38.933620
2412.457954	394979.209568	38.938637
2415.019168	395638.417871	38.943655
2417.029243	396303.709040	38.948672
2419.788978	396973.296635	38.953690
2422.248017	397638.635592	38.958708
2424.577710	398309.860193	38.963725
2427.198420	398982.516443	38.968743
2429.642478	399655.540978	38.973760
2432.197151	400310.412906	38.978778
2434.300730	400981.866074	38.983796
2436.646377	401649.462557	38.988813
2439.651839	402309.383450	38.993831
2441.380630	402988.376659	38.998848
2444.371758	403658.352980	39.003866
2446.631647	404338.315395	39.008884
2448.892072	405004.250035	39.013901
2451.362435	405675.555918	39.018919
2454.103253	406357.188303	39.023936
2456.462680	407031.291644	39.028954
2459.452765	407689.085855	39.033972
2461.599731	408378.163377	39.038989
2464.026004	409038.753927	39.044007
2466.590814	409715.163358	39.049024
2468.582076	410372.905071	39.054042
2471.078122	411014.411525	39.059060
2473.361811	411667.082883	39.064077
2475.461285	412299.758125	39.069095
2478.161831	412943.565124	39.074112
2480.416805	413597.991826	39.079130
2482.971280	414258.304772	39.084148
2484.933568	414923.080290	39.089165
2487.305384	415578.248439	39.094183
2489.278250	416248.306746	39.099200
2491.580408	416928.018134	39.104218
2494.195628	417612.370181	39.109236
2496.677336	418302.854250	39.114253
2499.305198	418990.054062	39.119271
2501.438492	419698.714235	39.124288
2503.670081	420394.019020	39.129306
2506.271635	421100.232777	39.134324
2508.592178	421818.753234	39.139341
2511.420756	422532.991354	39.144359
2513.214139	423265.685123	39.149376
2515.914813	423989.751163	39.154394
2518.743783	424713.015115	39.159412
2520.917025	425452.467119	39.164429
2523.411181	426185.717249	39.169447
2526.343644	426951.427864	39.174464
2528.743361	427691.077802	39.179482
2531.259088	428432.508327	39.184500
2533.615454	429190.040900	39.189517
2536.794412	429943.262454	39.194535
2538.928242	430701.745249	39.199552
2541.428243	431467.128782	39.204570
2544.179616	432231.180368	39.209588
2546.353992	433002.590957	39.214605
2549.085754	433764.115208	39.219623
2551.630586	434539.766398	39.224640
2554.470994	435326.983399	39.229658
2557.437646	436088.543790	39.234676
2559.409556	436880.203051	39.239693
2562.303174	437650.377243	39.244711
2564.716557	438431.686900	39.249728
2567.224803	439202.478922	39.254746
2569.916378	439992.645124	39.259764
2572.483956	440780.273811	39.264781
2575.347144	441572.834974	39.269799
2577.975573	442371.123798	39.274816
2580.541968	443152.191894	39.279834
2583.225555	443944.494913	39.284852
2585.897938	444746.079659	39.289869
2588.517473	445530.291650	39.294887
2590.867785	446310.523268	39.299904
2593.266390	447112.419605	39.304922
2596.141971	447914.409604	39.309940
2598.999515	448709.796907	39.314957
2601.644994	449504.987123	39.319975
2603.989345	450303.838721	39.324992
2606.662848	451098.357413	39.330010
2609.746365	451898.746069	39.335028
2612.047558	452703.582291	39.340045
2614.998078	453488.709836	39.345063
2617.516072	454293.145289	39.350080
2619.964491	455077.334585	39.355098
2622.924046	455878.196829	39.360116
2625.074657	456682.902768	39.365133
2628.208581	457485.645144	39.370151
2630.839295	458280.905679	39.375168
2633.103941	459079.936460	39.380186
2635.828047	459870.771139	39.385204
2638.296227	460685.325648	39.390221
2641.033409	461471.090318	39.395239
2643.502330	462251.611241	39.400256
2646.074511	463012.523159	39.405274
2648.833322	463780.501652	39.410292
2651.593996	464550.117729	39.415309
2654.306487	465316.325347	39.420327
2656.814075	466095.676542	39.425344
2658.980975	466868.937859	39.430362
2662.032116	467645.761950	39.435380
2663.952598	468428.653496	39.440397
2666.920612	469214.574265	39.445415
2669.583146	470001.018440	39.450432
2671.981767	470805.865022	39.455450
2674.381684	471594.711908	39.460468
2676.734392	472411.067802	39.465485
2679.401912	473209.705269	39.470503
2682.006321	474031.102314	39.475520
2684.572310	474857.622130	39.480538
2687.528985	475683.283159	39.485556
2689.814430	476520.534494	39.490573
2692.673130	477357.350315	39.495591
2695.378325	478200.214096	39.500608
2697.924759	479052.862957	39.505626
2700.681469	479889.327583	39.510644
2703.463316	480754.584254	39.515661
2705.883135	481608.497734	39.520679
2708.665215	482472.106851	39.525696
2711.344698	483337.559597	39.530714
2714.334702	484200.344386	39.535732
2717.079103	485084.180752	39.540749
2719.741207	485963.089815	39.545767
2722.404594	486834.786687	39.550784
2725.209661	487722.620777	39.555802
2728.175109	488603.619718	39.560820
2730.811519	489500.881066	39.565837
2733.576784	490373.243202	39.570855
2736.451133	491266.235581	39.575872
2739.238200	492160.710199	39.580890
2742.368423	493048.723379	39.585908
2744.462727	493948.568305	39.590925
2747.554528	494837.251938	39.595943
2750.345784	495726.544191	39.600960
2753.170453	496629.356043	39.605978
2756.203479	497529.714107	39.610996
2758.795687	498430.903833	39.616013
2761.578929	499342.102479	39.621031
2764.568365	500240.354717	39.626048
2767.148278	501149.722546	39.631066
2770.107720	502045.763546	39.636084
2773.111705	502961.669757	39.641101
2775.640920	503864.743400	39.646119
2778.395382	504768.183930	39.651136
2781.205242	505682.658793	39.656154
2783.999300	506590.025672	39.661172
2786.474847	507508.234384	39.666189
2789.229541	508422.210613	39.671207
2792.488509	509334.589665	39.676224
2795.601161	510257.577486	39.681242
2798.188473	511163.963913	39.686260
2800.914771	512087.917426	39.691277
2803.516790	512998.783356	39.696295
2806.814029	513913.715515	39.701312
2809.568195	514835.134633	39.706330
2812.119006	515737.383607	39.711348
2815.142972	516667.922432	39.716365
2817.828630	517569.135918	39.721383
2820.803678	518492.871743	39.726400
2823.550819	519405.908974	39.731418
2826.612936	520316.673719	39.736436
2829.155511	521190.695936	39.741453
2831.745989	522073.173122	39.746471
2834.720375	522937.050112	39.751488
2837.427516	523825.299389	39.756506
2840.406696	524697.838773	39.761524
2843.224967	525586.469535	39.766541
2845.640393	526455.021282	39.771559
2848.845828	527351.087435	39.776576
2851.186608	528246.084153	39.781594
2854.032841	529116.222268	39.786612
2857.107050	530025.289582	39.791629
2859.696638	530934.934497	39.796647
2862.715740	531824.970827	39.801664
2865.007132	532743.412458	39.806682
2868.083816	533661.767415	39.811700
2870.944264	534582.314513	39.816717
2873.784713	535507.939728	39.821735
2876.622560	536438.085447	39.826752
2879.246841	537381.440459	39.831770
2882.089189	538321.175225	39.836788
2885.326810	539264.556484	39.841805
2887.862841	540216.593948	39.846823
2891.076226	541157.790729	39.851840
2893.604297	542131.634496	39.856858
2896.418796	543083.030472	39.861876
2899.294270	544055.426150	39.866893
2902.355422	545030.640568	39.871911
2905.521964	545992.040283	39.876928
2908.085446	546974.995279	39.881946
2911.174532	547947.636700	39.886964
2914.181354	548931.234119	39.891981
2916.984518	549928.067339	39.896999
2920.042710	550907.894644	39.902016
2923.014664	551910.537679	39.907034
2926.298233	552896.015769	39.912052
2929.040165	553878.546065	39.917069
2932.173966	554864.206897	39.922087
2935.388723	555865.963649	39.927104
2938.272856	556863.378562	39.932122
2941.463648	557849.714831	39.937140
2944.482641	558853.088562	39.942157
2947.300072	559855.264113	39.947175
2950.422228	560855.806366	39.952192
2953.452655	561852.721335	39.957210
2956.314447	562849.839489	39.962228
2959.531865	563853.151034	39.967245
2962.472404	564840.109800	39.972263
2965.739178	565842.908172	39.977280
2968.785728	566834.919929	39.982298
2971.606901	567840.498733	39.987316
2974.520937	568835.541234	39.992333
2977.518104	569830.743723	39.997351
2980.812500	570831.541911	40.002368
2983.791606	571837.432894	40.007386
2986.945382	572836.992001	40.012404
2990.044096	573835.477439	40.017421
2992.628207	574839.739224	40.022439
2996.221475	575836.027213	40.027456
2998.734473	576822.028412	40.032474
3001.968264	577833.418339	40.037492
3005.004632	578825.545829	40.042509
3007.717515	579826.324796	40.047527
3011.298155	580825.776139	40.052544
3014.428682	581817.196263	40.057562
3016.950655	582821.323869	40.062580
3020.372200	583811.882570	40.067597
3023.132213	584811.745555	40.072615
3026.397004	585798.006798	40.077632
3028.932977	586765.358305	40.082650
3032.165646	587722.040846	40.087668
3035.249759	588663.985707	40.092685
3037.998981	589617.639701	40.097703
3040.842236	590573.006282	40.102720
3043.839984	591524.261930	40.107738
3046.422704	592486.934292	40.112756
3049.424774	593457.826510	40.117773
3052.275218	594435.327067	40.122791
3055.271040	595406.460668	40.127808
3058.083782	596411.705837	40.132826
3061.007184	597399.015731	40.137844
3064.049332	598391.731497	40.142861
3066.575979	599395.614816	40.147879
3069.600959	600421.361267	40.152896
3072.679195	601443.703345	40.157914
3075.906667	602470.936502	40.162932
3078.689614	603506.561075	40.167949
3081.459693	604547.149638	40.172967
3084.526685	605600.106984	40.177984
3087.563502	606663.631577	40.183002
3090.521435	607723.116122	40.188020
3093.700392	608792.822417	40.193037
3096.411177	609872.710728	40.198055
3099.690525	610957.103927	40.203072
3103.036894	612044.082131	40.208090
3106.115055	613129.798158	40.213108
3108.958223	614221.598342	40.218125
3111.997707	615334.761620	40.223143
3115.527916	616425.980830	40.228160
3118.171825	617551.335942	40.233178
3121.424849	618660.177790	40.238196
3124.741299	619786.492049	40.243213
3127.842606	620917.073706	40.248231
3131.097731	622031.869636	40.253248
3134.457807	623162.024499	40.258266
3137.643198	624285.843959	40.263284
3141.240459	625413.524836	40.268301
3144.104117	626555.595105	40.273319
3147.427648	627689.275586	40.278336
3150.947271	628812.414430	40.283354
3153.689703	629942.104527	40.288372
3157.341841	631067.279544	40.293389
3160.709803	632211.853480	40.298407
3163.761451	633340.279484	40.303424
3167.229162	634470.861404	40.308442
3170.569040	635603.088818	40.313460
3173.939426	636712.629870	40.318477
3176.863194	637847.326215	40.323495
3180.382671	638977.059612	40.328512
3183.522010	640100.794729	40.333530
3186.789363	641243.691380	40.338548
3190.006718	642346.365240	40.343565
3193.094163	643482.407077	40.348583
3196.500347	644600.366545	40.353600
3199.783525	645740.262566	40.358618
3202.563390	646862.961910	40.363636
3206.469002	647993.127494	40.368653
3209.209523	649127.196066	40.373671
3212.615152	650253.450712	40.378688
3216.074706	651385.300374	40.383706
3218.858134	652501.834993	40.388724
3222.481798	653624.682155	40.393741
3225.187022	654754.527692	40.398759
3229.008316	655872.254150	40.403776
3231.997905	656997.262302	40.408794
3235.055765	658142.548415	40.413812
3238.788556	659248.400019	40.418829
3241.557741	660331.630423	40.423847
3244.804270	661404.803940	40.428864
3247.700218	662485.831030	40.433882
3250.844242	663572.370238	40.438900
3254.447111	664660.353404	40.443917
3257.371769	665738.870150	40.448935
3260.523700	666821.258056	40.453952
3263.645197	667917.010509	40.458970
3266.486089	669016.364027	40.463988
3269.804394	670124.215683	40.469005
3272.667748	671239.522147	40.474023
3275.697406	672358.050644	40.479040
3279.315695	673493.303884	40.484058
3282.350703	674621.853807	40.489076
3285.510707	675759.293804	40.494093
3288.698046	676907.823208	40.499111
3291.857788	678057.606551	40.504128
3295.192981	679207.864093	40.509146
3298.286690	680389.269464	40.514164
3301.527404	681551.124470	40.519181
3304.743270	682742.937330	40.524199
3307.867718	683924.329198	40.529216
3311.657906	685104.415357	40.534234
3314.427396	686306.065446	40.539252
3317.794960	687504.478817	40.544269
3321.220629	688721.089901	40.549287
3324.488874	689929.968755	40.554304
3328.111914	691146.268563	40.559322
3330.752592	692370.801541	40.564340
3334.759075	693581.546088	40.569357
3338.023184	694818.687485	40.574375
3341.202810	696057.009213	40.579392
3344.947084	697282.368966	40.584410
3347.790275	698528.085742	40.589428
3351.807647	699773.878418	40.594445
3355.215727	701003.830837	40.599463
3358.353588	702245.846840	40.604480
3361.987000	703509.358773	40.609498
3365.430239	704749.925491	40.614516
3368.921875	705995.111635	40.619533
3372.092439	707253.198195	40.624551
3375.635918	708510.939917	40.629568
3379.109582	709759.347169	40.634586
3382.489638	711015.905288	40.639604
3386.210576	712270.884970	40.644621
3389.812315	713518.422364	40.649639
3393.248675	714773.770868	40.654656
3396.677025	716040.413768	40.659674
3400.090748	717289.304257	40.664692
3403.588838	718533.591933	40.669709
3406.913388	719796.072767	40.674727
3409.774165	721054.383382	40.679744
3413.515452	722305.089580	40.684762
3417.140055	723580.987776	40.689780
3420.746124	724829.751917	40.694797
3424.114841	726089.485731	40.699815
3427.500357	727357.769743	40.704832
3431.077893	728617.623581	40.709850
3434.110018	729882.263100	40.714868
3438.178551	731133.248361	40.719885
3441.501785	732405.250509	40.724903
3445.090242	733664.763038	40.729920
3448.642551	734925.121191	40.734938
3451.712974	736178.943789	40.739956
3455.350230	737437.905448	40.744973
3458.902548	738689.872639	40.749991
3462.260152	739943.500351	40.755008
3465.871937	741187.034879	40.760013
3468.996731	742391.837723	40.765018
3472.591031	743519.002533	40.770023
3475.646711	744612.874073	40.775028
3478.609240	745621.640592	40.780032
3481.995604	746567.440362	40.785037
3484.475602	747455.012101	40.790042
3487.573322	748268.707808	40.795047
3490.319612	749013.947320	40.800052
3492.635401	749694.221457	40.805056
3495.366019	750308.518753	40.810061
3497.251524	750871.584720	40.815066
3499.775499	751360.070449	40.820071
3501.759854	751803.175884	40.825076
3503.507887	752191.475313	40.830080
3505.945741	752508.428583	40.835085
3507.425993	752779.847142	40.840090
3509.367487	752996.317003	40.845095
3510.920620	753176.303072	40.850100
3512.405430	753316.743010	40.855104
3513.750685	753386.393622	40.860109
3514.655462	753440.018619	40.865114
3515.748330	753442.900136	40.870119
3516.926844	753424.485152	40.875124
3518.007714	753358.336301	40.880128
3519.133596	753281.167719	40.885133
3519.613326	753169.291448	40.890138
3520.624591	753032.536412	40.895143
3521.416594	752851.321272	40.900148
3521.964979	752663.524555	40.905152
3523.038788	752428.424252	40.910157
3523.222398	752215.391285	40.915162
3523.781150	751946.876777	40.920167
3524.310625	751680.580320	40.925172
3524.915474	751389.269852	40.930176
3525.423521	751076.379122	40.935181
3525.493077	750754.212098	40.940186
3525.968809	750428.210460	40.945191
3525.832763	750093.799028	40.950196
3526.015975	749754.281490	40.955200
3526.698357	749402.019204	40.960205
3526.626797	749029.361185	40.965210
3526.968092	748648.958765	40.970215
3526.934482	748269.439515	40.975220
3527.141436	747884.475936	40.980224
3527.453024	747483.415562	40.985229
3527.079423	747076.714781	40.990234
3527.428604	746679.461607	40.995239
3527.494173	746281.987840	41.000244
3527.178653	745866.021441	41.005248
3527.426096	745439.312726	41.010253
3527.288881	745038.398532	41.015258
3527.436398	744625.552501	41.020263
3527.516191	744204.242057	41.025268
3526.707247	743781.226160	41.030272
3527.029349	743351.820741	41.035277
3527.241900	742940.408214	41.040282
3527.350371	742502.437578	41.045287
3526.861765	742075.618065	41.050292
3526.705414	741645.555680	41.055296
3526.788559	741218.842926	41.060301
3526.595869	740803.330369	41.065306
3526.729518	740376.217654	41.070311
3526.548002	739950.964041	41.075316
3526.676116	739527.664765	41.080320
3526.433260	739086.891770	41.085325
3526.287022	738667.648411	41.090330
3526.081514	738233.995493	41.095335
3526.005116	737818.703409	41.100340
3525.971094	737395.070030	41.105344
3526.088276	736970.696494	41.110349
3525.495381	736551.316492	41.115354
3525.493791	736128.204430	41.120359
3525.519700	735713.082977	41.125364
3525.266813	735287.196422	41.130368
3524.947991	734877.582274	41.135373
3524.926805	734462.601859	41.140378
3524.788526	734037.521112	41.145383
3523.891350	733635.562114	41.150388
3524.030024	733236.778771	41.155392
3523.970728	732838.057834	41.160397
3523.881803	732450.907609	41.165402
3523.823946	732047.394354	41.170407
3523.540962	731655.039083	41.175412
3523.437941	731253.969472	41.180416
3523.231093	730848.836424	41.185421
3523.031369	730478.645155	41.190426
3522.968985	730080.036442	41.195431
3523.260016	729698.684611	41.200436
3522.863001	729317.081561	41.205440
3522.493268	728933.672957	41.210445
3522.004026	728562.451491	41.215450
3521.996557	728182.563871	41.220455
3522.316492	727806.419132	41.225460
3521.432304	727450.172924	41.230464
3521.758166	727065.372920	41.235469
3521.727024	726709.597957	41.240474
3521.691491	726348.060705	41.245479
3521.390424	725979.861994	41.250484
3521.072157	725621.064534	41.255488
3521.060941	725256.006488	41.260493
3520.681588	724909.081066	41.265498
3520.424350	724566.928079	41.270503
3520.113058	724204.102928	41.275508
3519.978798	723854.961576	41.280512
3519.734301	723513.109663	41.285517
3519.767245	723185.027070	41.290522
3519.347304	722843.424170	41.295527
3519.517204	722510.037896	41.300532
3519.157204	722182.475971	41.305536
3519.159274	721847.603482	41.310541
3518.980435	721524.199546	41.315546
3518.822753	721197.160255	41.320551
3518.740399	720873.913388	41.325556
3518.737926	720559.317753	41.330560
3518.591329	720235.412060	41.335565
3518.195627	719930.923116	41.340570
3518.076570	719605.798305	41.345575
3517.958129	719291.173842	41.350580
3517.617528	718985.847831	41.355584
3517.414771	718686.935132	41.360589
3517.410603	718391.897062	41.365594
3517.311889	718085.605556	41.370599
3517.406687	717788.595593	41.375604
3517.126040	717497.291457	41.380608
3517.067041	717195.176894	41.385613
3516.541928	716910.390576	41.390618
3516.501302	716627.151753	41.395623
3516.464707	716335.519003	41.400628
3516.270287	716058.933788	41.405632
3516.344361	715770.785469	41.410637
3516.224832	715501.263951	41.415642
3515.731077	715226.139438	41.420647
3515.903274	714945.785761	41.425652
3515.746302	714678.774504	41.430656
3515.500440	714400.108948	41.435661
3515.168286	714130.677868	41.440666
3514.982929	713876.299173	41.445671
3515.322516	713617.360186	41.450676
3514.714151	713359.760478	41.455680
3514.858398	713097.909889	41.460685
3514.459033	712845.719039	41.465690
3514.417192	712596.340294	41.470695
3514.553203	712355.461467	41.475700
3514.084452	712097.998899	41.480704
3514.264280	711843.647867	41.485709
3513.736628	711610.103823	41.490714
3513.811518	711372.334213	41.495719
3513.940036	711133.010333	41.500724
3513.766333	710892.339609	41.505728
3513.642600	710656.965443	41.510733
3513.382716	710420.465430	41.515738
3513.274811	710184.628825	41.520743
3513.439125	709959.662775	41.525748
3513.155375	709742.013001	41.530752
3513.144908	709494.424710	41.535757
3512.707908	709285.228670	41.540762
3512.882028	709058.797455	41.545767
3512.636245	708839.479970	41.550772
3512.576899	708628.716089	41.555776
3512.510914	708402.207759	41.560781
3512.135768	708195.656204	41.565786
3512.046561	707973.956947	41.570791
3512.227847	707763.777676	41.575796
3511.888891	707570.662369	41.580800
3512.220421	707353.645018	41.585805
3512.144955	707146.075265	41.590810
3511.951985	706944.082073	41.595815
3512.018512	706732.704582	41.600820
3511.665705	706541.306652	41.605824
3511.794343	706333.484994	41.610829
3511.460416	706129.161586	41.615834
3511.293769	705931.709681	41.620839
3511.200227	705733.893520	41.625844
3511.178872	705545.597698	41.630848
3511.036345	705349.817297	41.635853
3510.783895	705168.704065	41.640858
3510.740814	704977.071341	41.645863
3510.898415	704794.938900	41.650868
3510.546198	704598.083161	41.655872
3510.680508	704412.369819	41.660877
3510.459878	704243.800278	41.665882
3510.434203	704060.092865	41.670887
3510.216450	703872.140703	41.675892
3510.164775	703697.123920	41.680896
3510.210919	703529.043002	41.685901
3509.916626	703365.933559	41.690906
3509.718120	703195.203591	41.695911
3509.921113	703027.583955	41.700916
3509.591744	702856.868895	41.705920
3509.525388	702690.380227	41.710925
3509.527286	702538.386005	41.715930
3509.349061	702361.425313	41.720935
3509.432252	702206.132419	41.725940
3509.333349	702064.134165	41.730944
3509.537043	701890.877457	41.735949
3508.904461	701737.333964	41.740954
3509.087882	701578.137338	41.745959
3509.204063	701422.179014	41.750964
3508.756736	701271.131184	41.755968
3508.921322	701123.160451	41.760973
3508.860151	700977.560159	41.765978
3508.772335	700816.804033	41.770983
3508.734302	700668.809287	41.775988
3508.614747	700519.235085	41.780992
3508.737962	700377.769160	41.785997
3508.707358	700240.401777	41.791002
3508.264767	700099.819803	41.796007
3508.309051	699943.051681	41.801012
3508.471384	699804.701312	41.806016
3508.462495	699667.420760	41.811021
3507.864278	699534.658912	41.816026
3508.216522	699401.539612	41.821031
3508.007288	699250.666148	41.826036
3507.854971	699127.219197	41.831040
3507.867677	698984.655411	41.836045
3507.644944	698856.195723	41.841050
3507.936332	698730.035499	41.846055
3508.058838	698600.421570	41.851060
3507.880287	698464.790585	41.856064
3507.536648	698327.146522	41.861069
3507.529105	698199.586293	41.866074
3507.157779	698065.024864	41.871079
3507.409234	697959.192886	41.876084
3507.341049	697831.736741	41.881088
3507.391552	697701.475129	41.886093
3507.009078	697595.892386	41.891098
3506.976140	697468.922336	41.896103
3507.312971	697346.413811	41.901108
3507.264936	697237.092567	41.906112
3507.679453	697110.540803	41.911117
3507.248188	696996.904478	41.916122
3507.101489	696874.419349	41.921127
3507.180773	696746.276835	41.926132
3506.783844	696626.017202	41.931136
3506.941178	696515.161523	41.936141
3506.940516	696399.059878	41.941146
3506.639027	696294.890159	41.946151
3506.634984	696176.399423	41.951156
3506.607956	696067.259117	41.956160
3506.534930	695953.997848	41.961165
3506.566545	695840.270351	41.966170
3506.220314	695749.676732	41.971175
3506.651727	695638.018992	41.976180
3506.105729	695542.433735	41.981184
3506.516036	695426.500234	41.986189
3506.235406	695327.636594	41.991194
3506.340022	695222.840307	41.996199
3506.078315	695121.435048	42.001204
3506.014323	695023.228530	42.006208
3506.229265	694922.090561	42.011213
3506.050226	694825.094350	42.016218
3506.333924	694733.441628	42.021223
3506.380415	694630.488003	42.026228
3505.783320	694535.248417	42.031232
3505.851868	694432.189389	42.036237
3505.559401	694339.831801	42.041242
3505.756661	694247.193615	42.046247
3505.776037	694150.704416	42.051252
3505.491688	694071.522561	42.056256
3505.900524	693966.959723	42.061261
3505.809362	693881.179130	42.066266
3505.654630	693789.489437	42.071271
3505.746158	693697.012150	42.076276
3505.481440	693609.317753	42.081280
3505.410879	693513.880966	42.086285
3505.431321	693432.106502	42.091290
3505.413666	693342.080746	42.096295
3505.394540	693262.450059	42.101300
3505.119748	693168.137503	42.106304
3505.345777	693074.039871	42.111309
3505.131591	693020.503612	42.116314
3505.284160	692931.888167	42.121319
3505.217353	692853.952917	42.126324
3504.674414	692772.364712	42.131328
3505.210659	692681.494861	42.136333
3504.913971	692597.824993	42.141338
3504.647937	692515.392900	42.146343
3504.625274	692441.774543	42.151348
3504.590497	692374.425483	42.156352
3504.877786	692302.147769	42.161357
3504.760597	692233.269107	42.166362
3504.841113	692156.497391	42.171367
3505.117711	692079.841945	42.176372
3504.568974	692015.858166	42.181376
3504.851468	691917.858744	42.186381
3504.815597	691850.207423	42.191386
3505.057328	691774.450571	42.196391
3505.295089	691707.648557	42.201396
3504.668084	691628.998931	42.206400
3504.770547	691550.327910	42.211405
3504.750617	691483.019431	42.216410
3504.617452	691399.808887	42.221415
3504.783140	691317.443845	42.226420
3504.601853	691249.662687	42.231424
3505.001060	691188.750629	42.236429
3504.777539	691118.985364	42.241434
3504.563888	691031.655217	42.246439
3504.772152	690960.225475	42.251444
3504.390628	690900.584429	42.256448
3504.786603	690811.907847	42.261453
3504.426253	690746.640083	42.266458
3504.273244	690678.800187	42.271463
3504.776689	690606.920952	42.276468
3504.451932	690544.879935	42.281472
3504.406542	690475.975904	42.286477
3504.584111	690406.636554	42.291482
3504.101320	690339.744044	42.296487
3504.377870	690274.915217	42.301492
3504.404935	690219.033590	42.306496
3504.530194	690143.381649	42.311501
3504.403109	690088.519764	42.316506
3504.264821	690006.541068	42.321511
3504.417401	689939.789669	42.326516
3504.209833	689876.231948	42.331520
3504.483166	689793.088775	42.336525
3504.286725	689739.778735	42.341530
3504.030093	689677.073607	42.346535
3503.937945	689621.207903	42.351540
3503.894119	689560.059231	42.356544
3504.126770	689499.362197	42.361549
3504.058439	689443.989079	42.366554
3503.990790	689386.276698	42.371559
3504.210314	689321.301102	42.376564
3503.787522	689266.383395	42.381568
3504.474287	689197.946062	42.386573
3504.102024	689140.282297	42.391578
3503.907197	689071.790220	42.396583
3504.060531	689010.754615	42.401588
3503.800660	688949.040219	42.406592
3503.903709	688897.566876	42.411597
3503.746926	688844.593343	42.416602
3503.794181	688783.922034	42.421607
3503.864286	688730.761148	42.426612
3503.877123	688681.739947	42.431616
3503.949886	688629.125447	42.436621
3504.091510	688562.315865	42.441626
3503.685483	688506.494958	42.446631
3504.087407	688444.070848	42.451636
3503.638158	688387.111678	42.456640
3504.046638	688325.531714	42.461645
3503.767472	688274.764776	42.466650
3503.564641	688216.768563	42.471655
3504.083225	688156.562818	42.476660
3503.886981	688117.327658	42.481664
3503.909327	688055.859250	42.486669
3503.624930	688001.259399	42.491674
3503.836789	687940.057592	42.496679
3503.691405	687890.062760	42.501684
3503.569487	687848.275902	42.506688
3503.735631	687790.365459	42.511693
3503.811391	687723.411205	42.516698
3504.074094	687677.926892	42.521703
3503.819862	687612.569103	42.526708
3503.764277	687562.706976	42.531712
3504.116871	687518.849525	42.536717
3503.992924	687444.211414	42.541722
3503.855130	687387.941197	42.546727
3503.816325	687321.799212	42.551732
3503.465839	687281.441046	42.556736
3503.243155	687221.848957	42.561741
3503.654555	687186.541303	42.566746
3503.602156	687128.911502	42.571751
3503.636386	687086.995844	42.576756
3503.390416	687021.532867	42.581760
3503.465075	686971.596241	42.586765
3503.465263	686929.984116	42.591770
3503.122466	686875.038648	42.596775
3503.484786	686824.605828	42.601780
3503.153844	686785.337298	42.606784
3503.218180	686739.283638	42.611789
3503.107275	686707.594313	42.616794
3503.051917	686664.247935	42.621799
3503.291078	686608.707184	42.626804
3503.304872	686570.973788	42.631808
3503.388784	686515.507826	42.636813
3503.400015	686473.493560	42.641818
3503.136283	686425.799914	42.646823
3503.432043	686383.788126	42.651828
3502.988003	686346.378129	42.656832
3503.164723	686281.586827	42.661837
3503.358537	686245.763795	42.666842
3503.178814	686203.381508	42.671847
3503.264549	686150.053525	42.676852
3503.229542	686109.837262	42.681856
3503.474803	686066.936290	42.686861
3503.304753	686025.248499	42.691866
3503.227050	685969.706267	42.696871
3503.368031	685920.200944	42.701876
3503.200481	685885.829904	42.706880
3503.380196	685830.543090	42.711885
3503.691017	685791.512968	42.716890
3503.140034	685745.655215	42.721895
3503.078920	685693.394167	42.726900
3502.891048	685652.255202	42.731904
3503.172540	685600.833250	42.736909
3503.000070	685567.059205	42.741914
3503.148171	685529.299343	42.746919
3503.425475	685489.775617	42.751924
3503.173140	685442.124699	42.756928
3503.498183	685396.568882	42.761933
3503.117946	685357.202712	42.766938
3502.989898	685303.805416	42.771943
3503.540312	685265.579891	42.776948
3503.155864	685220.837087	42.781952
3503.019600	685168.784541	42.786957
3503.050771	685130.195942	42.791962
3502.688480	685091.074587	42.796967
3503.276585	685047.017023	42.801972
3502.973602	685006.541316	42.806977
3502.997062	684970.492395	42.811981
3503.170691	684933.572219	42.816986
3502.948518	684887.904878	42.821991
3503.007750	684835.867999	42.826996
3502.621762	684807.503301	42.832001
3502.916095	684762.098728	42.837005
3503.189459	684742.586897	42.842010
3502.830927	684699.729177	42.847015
3503.419917	684653.678059	42.852020
3502.817716	684621.415159	42.857025
3503.151961	684570.078265	42.862029
3503.503436	684521.377043	42.867034
3503.213475	684484.033547	42.872039
3503.349485	684428.994358	42.877044
3502.968633	684385.989470	42.882049
3502.981635	684353.375297	42.887053
3503.245750	684309.666295	42.892058
3503.016792	684276.892560	42.897063
3503.264574	684225.269231	42.902068
3503.094744	684185.863315	42.907073
3503.253856	684144.809721	42.912077
3503.019236	684094.161374	42.917082
3502.845895	684063.668091	42.922087
3503.047817	684015.885054	42.927092
3502.874763	683980.711051	42.932097
3502.914172	683938.132711	42.937101
3503.067795	683913.560069	42.942106
3502.900112	683866.982371	42.947111
3503.264464	683827.835429	42.952116
3503.045331	683787.689027	42.957121
3502.933500	683749.566276	42.962125
3502.933254	683705.997529	42.967130
3502.977167	683675.865495	42.972135
3502.830280	683623.905451	42.977140
3502.863268	683594.322677	42.982145
3503.024826	683543.357017	42.987149
3503.181408	683514.301352	42.992154
3502.946896	683470.023169	42.997159
3503.163122	683418.201298	43.002164
3502.978923	683396.322049	43.007169
3502.861248	683337.334490	43.012173
3502.885936	683311.835367	43.017178
3502.917320	683269.006252	43.022183
3503.309398	683229.652998	43.027188
3502.978692	683182.849691	43.032193
3503.000147	683146.246131	43.037197
3503.176321	683104.487902	43.042202
3502.927325	683067.131847	43.047207
3503.089564	683027.218036	43.052212
3503.113790	682993.601217	43.057217
3503.090914	682944.803881	43.062221
3503.049338	682910.948614	43.067226
3502.986815	682873.561041	43.072231
3503.179742	682818.502762	43.077236
3502.923003	682786.674408	43.082241
3502.870191	682748.288760	43.087245
3502.930553	682712.175034	43.092250
3502.967436	682676.363827	43.097255
3503.031596	682617.839648	43.102260
3503.020132	682597.473790	43.107265
3502.661051	682552.514497	43.112269
3502.856033	682513.937635	43.117274
3502.781103	682478.691875	43.122279
3502.725112	682435.325455	43.127284
3502.978431	682410.582946	43.132289
3502.923435	682367.016838	43.137293
3502.866283	682326.389116	43.142298
3502.776999	682294.929860	43.147303
3502.959627	682250.577030	43.152308
3502.810809	682224.406252	43.157313
3502.862977	682190.582673	43.162317
3502.837395	682149.152141	43.167322
3502.900375	682115.276701	43.172327
3502.823249	682075.846401	43.177332
3502.929951	682043.656760	43.182337
3502.863886	682004.124724	43.187341
3503.067248	681966.241410	43.192346
3502.647679	681930.303289	43.197351
3502.921867	681881.451334	43.202356
3502.523180	681863.189576	43.207361
3502.669763	681828.054219	43.212365
3502.808116	681783.507212	43.217370
3502.748827	681751.343897	43.222375
3502.524222	681715.572022	43.227380
3502.565106	681688.721002	43.232385
3502.969990	681652.496525	43.237389
3502.702212	681618.125904	43.242394
3502.528419	681577.215252	43.247399
3502.467496	681554.713624	43.252404
3502.916569	681523.710863	43.257409
3502.969322	681478.877653	43.262413
3502.780729	681439.164151	43.267418
3502.569185	681416.587392	43.272423
3502.809063	681370.079231	43.277428
3502.926109	681351.283215	43.282433
3502.920204	681305.512511	43.287437
3502.869862	681260.446191	43.292442
3502.821306	681234.554902	43.297447
3503.064017	681190.286660	43.302452
3502.520769	681147.094050	43.307457
3502.953193	681115.843623	43.312461
3503.154317	681074.819145	43.317466
3502.832901	681052.807478	43.322471
3503.050634	681004.906507	43.327476
3503.037599	680964.713752	43.332481
3503.002488	680923.677720	43.337485
3503.119576	680886.202633	43.342490
3502.751667	680844.822619	43.347495
3503.053078	680811.550592	43.352500
3503.017920	680773.851091	43.357505
3503.220122	680726.947413	43.362509
3503.200598	680685.808131	43.367514
3502.763313	680642.097586	43.372519
3503.071716	680605.087927	43.377524
3502.907615	680582.152628	43.382529
3502.793906	680541.327080	43.387533
3503.196744	680498.075138	43.392538
3502.659753	680463.694743	43.397543
3502.959819	680430.172506	43.402548
3502.741788	680391.953653	43.407553
3502.542296	680356.670454	43.412557
3502.757799	680321.617605	43.417562
3502.593739	680294.049109	43.422567
3502.515833	680253.515253	43.427572
3502.537060	680233.587070	43.432577
3502.606723	680196.116988	43.437581
3503.037335	680158.138965	43.442586
3502.656624	680124.727796	43.447591
3502.575300	680086.435334	43.452596
3502.728321	680057.219869	43.457601
3502.549127	680018.943253	43.462605
3502.766107	679986.877677	43.467610
3502.384207	679956.903213	43.472615
3502.765704	679910.713036	43.477620
3502.649045	679884.480472	43.482625
3502.857601	679860.934015	43.487629
3503.127407	679819.045787	43.492634
3502.821943	679781.685648	43.497639
3503.010862	679740.208906	43.502644
3502.729971	679711.014031	43.507649
3502.641475	679671.176765	43.512653
3502.733950	679641.272550	43.517658
3502.856098	679609.520180	43.522663
3502.589496	679567.818832	43.527668
3502.943522	679534.184817	43.532673
3502.810371	679497.343104	43.537677
3503.077054	679463.125431	43.542682
3502.389924	679424.680963	43.547687
3502.496361	679403.342085	43.552692
3502.540527	679366.620081	43.557697
3502.605694	679334.328170	43.562701
3502.945132	679298.304491	43.567706
3502.262573	679267.630069	43.572711
3503.220208	679229.312298	43.577716
3502.831363	679202.674287	43.582721
3502.711586	679170.063554	43.587725
3503.033408	679127.416352	43.592730
3502.716175	679096.133162	43.597735
3502.601575	679049.472426	43.602740
3502.934326	679024.558275	43.607745
3502.876798	678991.687562	43.612749
3503.009758	678948.124098	43.617754
3502.487783	678917.123133	43.622759
3502.936962	678874.852332	43.627764
3503.078903	678841.848579	43.632769
3503.177190	678804.119030	43.637773
3503.169960	678765.908515	43.642778
3502.762775	678733.094498	43.647783
3503.198030	678691.672098	43.652788
3502.890356	678646.884494	43.657793
3502.661965	678608.361027	43.662797
3503.166864	678575.396156	43.667802
3502.613281	678543.950755	43.672807
3502.682229	678502.338762	43.677812
3502.709171	678448.278107	43.682817
3502.799496	678433.715385	43.687821
3502.866523	678383.583659	43.692826
3502.376568	678360.895812	43.697831
3502.976712	678318.497953	43.702836
3502.816176	678285.591880	43.707841
3502.598016	678261.613440	43.712845
3503.064390	678213.208601	43.717850
3502.809200	678182.958373	43.722855
3502.613365	678145.075310	43.727860
3503.114881	678109.070120	43.732865
3503.050877	678083.072876	43.737869
3502.760615	678040.969941	43.742874
3502.498232	678011.168750	43.747879
3502.900289	677966.808965	43.752884
3503.061356	677937.485826	43.757889
3502.750996	677895.136417	43.762893
3503.037921	677856.375429	43.767898
3502.857008	677826.908993	43.772903
3502.775608	677776.648965	43.777908
3502.782720	677755.571781	43.782913
3502.847216	677715.152793	43.787917
3502.915516	677672.889447	43.792922
3502.671248	677647.319291	43.797927
3502.818312	677601.654478	43.802932
3502.571764	677577.579290	43.807937
3502.853942	677546.989302	43.812941
3502.952029	677493.559095	43.817946
3502.536572	677478.181333	43.822951
3502.945588	677429.482897	43.827956
3502.669943	677403.120003	43.832961
3502.823635	677359.495823	43.837965
3502.727082	677327.622178	43.842970
3502.742551	677306.293458	43.847975
3502.994486	677261.107966	43.852980
3502.790100	677226.710515	43.857985
3502.829299	677193.269365	43.862989
3502.521989	677156.098223	43.867994
3502.439975	677120.484327	43.872999
3502.909201	677098.781386	43.878004
3502.754888	677057.100036	43.883009
3502.877988	677022.598035	43.888013
3502.877891	676986.970129	43.893018
3502.936714	676948.940553	43.898023
3503.104295	676909.746812	43.903028
3502.463784	676873.177569	43.908033
3502.639907	676840.310547	43.913037
3502.989703	676796.751070	43.918042
3502.293130	676766.419455	43.923047
3502.625162	676743.243373	43.928052
3502.632259	676715.984810	43.933057
3502.581788	676683.852207	43.938061
3502.682533	676639.784891	43.943066
3502.745448	676612.865648	43.948071
3503.191659	676576.066331	43.953076
3502.904281	676538.739935	43.958081
3502.875338	676510.240910	43.963085
3503.153471	676473.369219	43.968090
3502.757603	676440.395709	43.973095
3502.783034	676396.788144	43.978100
3502.949018	676365.565593	43.983105
3502.927375	676322.413932	43.988109
3502.913192	676282.001671	43.993114
3502.698683	676260.658613	43.998119
3503.056740	676211.115028	44.003124
3503.219344	676183.380777	44.008129
3502.911768	676139.428209	44.013133
3502.641373	676095.967649	44.018138
3502.998877	676069.795640	44.023143
3502.727324	676023.843213	44.028148
3502.698709	675988.315849	44.033153
3502.752867	675945.598463	44.038157
3502.880560	675916.872470	44.043162
3502.620121	675880.535696	44.048167
3503.075631	675845.974557	44.053172
3502.785052	675807.948055	44.058177
3502.656233	675778.915055	44.063181
3502.837968	675737.870117	44.068186
3502.615555	675711.194627	44.073191
3502.649066	675683.430324	44.078196
3502.592334	675642.822954	44.083201
3502.750987	675623.360573	44.088205
3502.833339	675578.095180	44.093210
3502.752229	675552.542203	44.098215
3502.942842	675515.681145	44.103220
3502.713149	675482.726691	44.108225
3502.737921	675442.404043	44.113229
3502.891547	675407.043782	44.118234
3502.429811	675375.572485	44.123239
3502.584772	675335.576789	44.128244
3502.541867	675306.677674	44.133249
3502.765901	675271.105943	44.138253
3502.705088	675233.089071	44.143258
3502.797238	675208.902090	44.148263
3502.612331	675169.161041	44.153268
3502.831610	675125.116867	44.158273
3502.747159	675110.179024	44.163277
3502.806673	675066.858656	44.168282
3502.391494	675034.082699	44.173287
3502.656696	674991.326165	44.178292
3502.679249	674957.630526	44.183297
3502.273887	674930.883268	44.188301
3502.621938	674895.189988	44.193306
3502.524642	674878.160582	44.198311
3502.940141	674843.801693	44.203316
3502.928063	674802.485533	44.208321
3502.751118	674781.382098	44.213325
3502.866431	674738.100851	44.218330
3502.720801	674706.126629	44.223335
3503.035164	674665.304330	44.228340
3502.409138	674637.496068	44.233345
3502.526979	674595.609322	44.238349
3502.894046	674568.335003	44.243354
3502.783578	674540.890080	44.248359
3502.935851	674493.863419	44.253364
3502.596765	674463.365686	44.258369
3502.847148	674436.857856	44.263373
3502.789963	674394.650149	44.268378
3502.999634	674355.039987	44.273383
3503.042405	674321.737472	44.278388
3503.112607	674279.857162	44.283393
3502.710913	674256.696129	44.288397
3503.086006	674201.257471	44.293402
3502.785966	674166.465717	44.298407
3502.780806	674128.385332	44.303412
3502.745122	674094.098040	44.308417
3502.577514	674060.480347	44.313421
3502.989677	674028.561428	44.318426
3502.570474	673999.271667	44.323431
3502.767808	673956.471743	44.328436
3502.834568	673928.297978	44.333441
3502.956978	673887.653456	44.338445
3503.064788	673848.556397	44.343450
3502.568659	673815.639960	44.348455
3502.737171	673775.685204	44.353460
3502.866049	673735.038954	44.358465
3502.394366	673715.377390	44.363469
3502.639883	673668.480758	44.368474
3502.493542	673658.485665	44.373479
3502.829176	673616.458954	44.378484
3502.857962	673575.280182	44.383489
3502.449643	673540.603636	44.388493
3503.409352	673502.710651	44.393498
3502.564024	673464.267529	44.398503
3503.024008	673438.270668	44.403508
3502.830601	673401.614104	44.408513
3502.502411	673370.612522	44.413517
3502.604167	673324.684988	44.418522
3502.553328	673302.909397	44.423527
3503.057405	673258.111622	44.428532
3502.544583	673228.934572	44.433537
3502.815008	673201.123859	44.438541
3502.813904	673167.674921	44.443546
3502.444404	673132.641518	44.448551
3502.366389	673104.688534	44.453556
3502.505148	673063.439542	44.458561
3502.450917	673030.148420	44.463565
3502.568424	673002.810973	44.468570
3502.522048	672984.722862	44.473575
3502.665547	672942.824498	44.478580
3502.518414	672917.374899	44.483585
3502.289522	672886.804013	44.488589
3502.943362	672853.495291	44.493594
3502.803544	672828.393206	44.498599
3502.719661	672791.367246	44.503604
3502.491866	672751.622990	44.508609
3502.433979	672723.216884	44.513613
3502.723944	672680.495580	44.518618
3502.617322	672658.328865	44.523623
3502.631360	672618.594048	44.528628
3502.306673	672587.838563	44.533633
3502.272342	672551.501433	44.538637
3502.600044	672527.368420	44.543642
3502.216984	672502.106131	44.548647
3502.326770	672462.953119	44.553652
3502.444150	672442.992396	44.558657
3502.314740	672413.550212	44.563661
3502.404044	672396.286125	44.568666
3502.275180	672366.345163	44.573671
3502.473212	672336.200676	44.578676
3502.628170	672310.250963	44.583681
3502.243389	672279.105532	44.588685
3502.648318	672249.325511	44.593690
3502.642357	672215.724419	44.598695
3502.342714	672192.092761	44.603700
3502.520214	672151.581209	44.608705
3502.623791	672117.263742	44.613709
3502.613453	672093.235175	44.618714
3502.431064	672053.929184	44.623719
3502.755174	672030.992031	44.628724
3502.784870	671991.700688	44.633729
3502.772580	671968.669247	44.638733
3502.820457	671934.160866	44.643738
3502.594911	671895.908311	44.648743
3502.585436	671855.875006	44.653748
3502.610089	671832.388433	44.658753
3502.524177	671796.804741	44.663757
3502.663804	671759.139598	44.668762
3502.656686	671739.048326	44.673767
3502.459511	671694.059516	44.678772
3502.828564	671681.733790	44.683777
3502.683671	671646.358680	44.688781
3502.602246	671599.405884	44.693786
3502.935114	671570.383466	44.698791
3502.777768	671538.200935	44.703796
3503.149992	671500.496431	44.708801
3502.768526	671462.367523	44.713805
3503.017987	671423.536186	44.718810
3502.641443	671387.749544	44.723815
3502.863950	671357.099298	44.728820
3502.743103	671328.400198	44.733825
3502.559711	671290.287813	44.738829
3502.696656	671246.887184	44.743834
3502.737961	671227.235582	44.748839
3502.373021	671187.258010	44.753844
3502.639872	671150.815983	44.758849
3502.082846	671127.224059	44.763853
3502.283724	671095.379871	44.768858
3502.286879	671073.440635	44.773863
3502.571440	671036.945389	44.778868
3502.288666	671017.147307	44.783873
3502.238095	670981.903742	44.788877
3502.247433	670952.882876	44.793882
3502.296449	670930.038241	44.798887
3502.338220	670900.862286	44.803892
3502.525281	670874.604160	44.808897
3502.412050	670846.450820	44.813901
3502.708809	670805.514935	44.818906
3502.211201	670785.951217	44.823911
3502.768151	670752.152423	44.828916
3502.707490	670728.278256	44.833921
3502.402223	670700.106259	44.838925
3502.478895	670669.976444	44.843930
3502.730598	670634.931090	44.848935
3502.783359	670594.981903	44.853940
3502.582687	670559.212995	44.858945
3502.440186	670537.196786	44.863949
3502.865477	670503.668120	44.868954
3502.760206	670478.803393	44.873959
3502.814491	670438.504244	44.878964
3502.886371	670401.592812	44.883969
3502.459289	670372.492484	44.888973
3502.951441	670329.428025	44.893978
3502.610760	670295.476325	44.898983
3502.516441	670255.649669	44.903988
3502.833577	670227.273969	44.908993
3502.667980	670198.778268	44.913997
3502.581189	670162.241106	44.919002
3502.552650	670135.418066	44.924007
3502.413492	670105.072685	44.929012
3502.714576	670063.135554	44.934017
3502.385296	670044.240684	44.939021
3502.520834	670007.217490	44.944026
3502.523992	669978.743184	44.949031
3502.250036	669944.280558	44.954036
3502.403961	669910.096370	44.959041
3502.456250	669901.560560	44.964045
3502.793868	669863.705631	44.969050
3502.469571	669842.814843	44.974055
3502.646230	669812.067409	44.979060
3502.682218	669759.650541	44.984065
3502.228372	669729.954226	44.989069
3502.698575	669701.202652	44.994074
3502.708139	669680.655436	44.999079
3502.515057	669646.776819	45.004084
3502.448348	669600.060997	45.009089
3502.522782	669576.261397	45.014093
3502.518738	669543.348636	45.019098
3502.198729	669510.737174	45.024103
3502.190178	669491.838217	45.029108
3502.645734	669455.558043	45.034113
3502.419563	669440.135839	45.039117
3502.534145	669393.389124	45.044122
3502.110886	669378.747343	45.049127
3502.392481	669338.904754	45.054132
3502.340733	669316.222436	45.059137
3502.361949	669291.084392	45.064141
3502.428740	669267.434886	45.069146
3502.196973	669240.243833	45.074151
3502.481844	669218.952061	45.079156
3502.306313	669182.974320	45.084161
3502.391777	669159.770307	45.089165
3502.570083	669122.936095	45.094170
3502.031171	669085.621467	45.099175
3502.280808	669071.666273	45.104180
3502.021652	669052.009790	45.109185
3502.166983	669026.601234	45.114189
3502.541427	668998.262287	45.119194
3502.529319	668973.976716	45.124199
3502.154368	668936.434994	45.129204
3502.440397	668914.693499	45.134209
3502.550874	668886.248098	45.139213
3502.515822	668856.230666	45.144218
3502.332437	668824.641652	45.149223
3502.364997	668806.482648	45.154228
3502.446934	668767.069542	45.159233
3502.218830	668749.352366	45.164237
3502.297008	668717.919389	45.169242
3502.490755	668695.245005	45.174247
3502.276811	668660.318953	45.179252
3502.163064	668644.378189	45.184257
3502.391127	668609.877855	45.189261
3502.291234	668585.356385	45.194266
3502.452993	668558.896516	45.199271
3502.348143	668537.966684	45.204276
3502.147230	668495.706349	45.209281
3502.018883	668481.313828	45.214285
3502.346141	668433.679471	45.219290
3501.916729	668431.954822	45.224295
3501.979802	668403.815036	45.229300
3501.992499	668379.174731	45.234305
3501.867728	668370.467220	45.239309
3502.091333	668332.924226	45.244314
3502.101048	668319.007463	45.249319
3502.034567	668290.888691	45.254324
3502.046258	668263.854222	45.259329
3502.194394	668259.341078	45.264333
3502.059235	668218.365444	45.269338
3502.228804	668212.402343	45.274343
3502.245357	668186.164868	45.279348
3502.319020	668160.267044	45.284353
3502.181321	668125.426213	45.289357
3502.246654	668108.557263	45.294362
3501.834472	668086.280533	45.299367
3502.252143	668057.432893	45.304372
3502.149580	668042.835951	45.309377
3501.784789	668020.601135	45.314381
3501.893871	667998.188426	45.319386
3502.203879	667980.281387	45.324391
3502.022957	667956.719314	45.329396
3502.294274	667934.080211	45.334401
3502.161920	667910.410265	45.339405
3502.164046	667887.416388	45.344410
3502.322762	667852.176567	45.349415
3502.256745	667830.540486	45.354420
3502.023162	667800.552433	45.359425
3502.053955	667790.621679	45.364429
3502.390463	667755.751230	45.369434
3502.057587	667732.512911	45.374439
3502.042307	667703.236757	45.379444
3502.328250	667670.519113	45.384449
3502.165068	667649.796451	45.389453
3502.204846	667622.007345	45.394458
3502.245658	667612.573545	45.399463
3501.878196	667579.364708	45.404468
3502.170005	667549.189528	45.409473
3502.046744	667530.355449	45.414477
3502.271810	667513.459124	45.419482
3502.280466	667486.123666	45.424487
3502.241367	667462.237718	45.429492
3502.186431	667441.446886	45.434497
3502.021178	667417.332213	45.439501
3502.199738	667398.398258	45.444506
3502.108199	667365.791651	45.449511
3502.232592	667341.080371	45.454516
3502.295510	667321.666514	45.459521
3501.975699	667322.068465	45.464525
3501.907797	667284.020685	45.469530
3502.306742	667261.009788	45.474535
3502.115253	667239.742206	45.479540
3502.047168	667215.361604	45.484545
3502.147078	667195.741869	45.489549
3501.963254	667157.962094	45.494554
3501.934987	667148.688863	45.499559
3501.997612	667137.555024	45.504564
3501.827397	667102.017459	45.509569
3501.743980	667103.477866	45.514573
3502.020024	667074.002127	45.519578
3502.085799	667041.767545	45.524583
3502.165965	667026.590229	45.529588
3502.107362	666987.841382	45.534593
3501.960531	666984.473656	45.539597
3502.377522	666948.489581	45.544602
3502.029603	666937.921986	45.549607
3501.670675	666913.339123	45.554612
3502.043613	666882.051043	45.559617
3501.872546	666876.542303	45.564621
3502.053753	666852.618525	45.569626
3501.900215	666819.571317	45.574631
3502.173701	666803.114706	45.579636
3502.086315	666785.769746	45.584641
3501.897353	666779.615413	45.589645
3502.078200	666746.113781	45.594650
3502.071709	666720.175367	45.599655
3501.669977	666697.744007	45.604660
3501.953092	666666.370254	45.609665
3502.199712	666656.003680	45.614669
3502.117545	666637.610022	45.619674
3502.084457	666618.659513	45.624679
3501.940866	666595.686531	45.629684
3502.383184	666564.435864	45.634689
3501.980061	666556.520828	45.639693
3502.153435	666524.216883	45.644698
3502.227265	666501.656811	45.649703
3502.293653	666479.596764	45.654708
3502.460008	666456.622258	45.659713
3502.174242	666429.282402	45.664717
3502.541703	666403.680591	45.669722
3502.353632	666382.460418	45.674727
3502.511594	666351.954312	45.679732
3502.401941	666310.217979	45.684737
3501.966272	666299.364816	45.689741
3502.113671	666265.268378	45.694746
3502.105008	666242.621516	45.699751
3501.876574	666227.693328	45.704756
3502.522316	666196.507712	45.709761
3502.284655	666179.884825	45.714765
3502.501945	666145.377349	45.719770
3502.385899	666129.981507	45.724775
3501.861188	666105.124555	45.729780
3502.134098	666079.088472	45.734785
3501.994605	666059.705403	45.739789
3502.331944	666032.062182	45.744794
3502.442923	665999.916410	45.749799
3502.420785	665982.010474	45.754804
3502.426522	665953.872905	45.759809
3502.173071	665929.170346	45.764813
3502.287552	665879.961887	45.769818
3502.287751	665794.902107	45.774823
3502.211360	665660.314155	45.779828
3502.191470	665469.837935	45.784833
3501.793589	665222.444094	45.789837
3502.099522	664914.507322	45.794842
3501.483710	664548.934113	45.799847
3501.112596	664134.606985	45.804852
3501.137990	663657.373002	45.809857
3500.750499	663126.787803	45.814861
3500.578709	662533.905729	45.819866
3500.326086	661893.687003	45.824871
3499.579514	661190.368094	45.829876
3499.532035	660411.758766	45.834881
3498.619533	659590.197906	45.839885
3498.411765	658709.939246	45.844890
3497.811421	657777.588902	45.849895
3496.974804	656784.267899	45.854900
3496.664476	655725.687231	45.859905
3495.783789	654610.747455	45.864909
3495.062941	653445.004008	45.869914
3494.268290	652223.581968	45.874919
3493.261738	650927.797239	45.879924
3492.467814	649587.434375	45.884929
3491.512443	648200.438681	45.889933
3490.282477	646728.621217	45.894938
3489.338623	645225.945935	45.899943
3487.967921	643669.967226	45.904948
3487.137859	642038.698384	45.909953
3485.690450	640371.108565	45.914957
3484.461871	638653.136496	45.919962
3483.114718	636869.653745	45.924967
3481.587111	635039.003912	45.929972
3480.690744	633163.582685	45.934977
3479.089146	631243.037461	45.939981
3477.899971	629249.772856	45.944986
3476.500807	627214.601658	45.949991
3474.882859	625128.337212	45.954996
3473.545134	622997.583272	45.960001
3471.389420	620827.457997	45.965005
3469.910398	618591.631898	45.970010
3468.040947	616335.962435	45.975015
3466.224092	614023.865200	45.980020
3464.511382	611667.988030	45.985025
3462.083440	609281.383614	45.990029
3460.316406	606841.181351	45.995034
3458.343783	604360.992845	46.000039
3456.290472	601850.714152	46.005044
3454.445205	599290.049366	46.010049
3452.325596	596708.727450	46.015053
3450.127935	594071.798465	46.020058
3447.446102	591399.895200	46.025063
3445.356892	588693.223747	46.030068
3443.208581	585959.362505	46.035073
3440.544768	583202.144335	46.040077
3438.082575	580380.458372	46.045082
3435.581446	577542.842531	46.050087
3433.115748	574670.615442	46.055092
3430.914260	571768.955297	46.060097
3428.066388	568836.740268	46.065101
3425.489550	565881.406667	46.070106
3422.913098	562889.746941	46.075111
3419.936521	559875.660008	46.080116
3417.357379	556830.643642	46.085121
3414.446409	553769.719655	46.090125
3411.819049	550676.705595	46.095130
3408.898476	547561.512957	46.100135
3405.886740	544424.101416	46.105140
3403.150304	541249.878506	46.110145
3400.156621	538068.527595	46.115149
3397.587734	534858.747904	46.120154
3394.261524	531624.357826	46.125159
3391.203907	528376.033944	46.130164
3388.268717	525096.077945	46.135169
3384.980669	521806.474506	46.140173
3381.750910	518489.782521	46.145178
3378.716482	515162.139012	46.150183
3375.096270	511815.084545	46.155188
3371.889186	508451.990030	46.160193
3368.680228	505085.107637	46.165197
3365.370598	501695.499019	46.170202
3362.081901	498289.411676	46.175207
3358.597483	494883.625674	46.180212
3355.703357	491439.517818	46.185217
3352.034504	488002.188909	46.190221
3348.721439	484540.034169	46.195226
3345.188551	481059.624855	46.200231
3341.480464	477588.601192	46.205236
3338.205082	474092.592052	46.210241
3334.410623	470593.178324	46.215245
3331.030083	467079.930444	46.220250
3327.569320	463567.831421	46.225255
3323.659055	460035.363145	46.230260
3320.363562	456499.991126	46.235265
3316.579262	452963.073197	46.240269
3312.799946	449412.368361	46.245274
3309.362683	445858.476027	46.250279
3305.826987	442294.884376	46.255284
3302.034402	438728.272334	46.260289
3298.194079	435165.820733	46.265293
3294.649874	431575.514297	46.270298
3291.159463	428002.413159	46.275303
3287.004511	424417.160942	46.280308
3283.197974	420829.116542	46.285313
3279.401482	417247.004003	46.290317
3275.833282	413652.061383	46.295322
3271.922213	410058.992152	46.300327
3268.215839	406454.942300	46.305332
3264.320274	402860.484467	46.310337
3260.860196	399270.830836	46.315341
3256.500561	395660.373480	46.320346
3253.178875	392064.450765	46.325351
3249.010425	388466.870228	46.330356
3245.277934	384863.059416	46.335361
3241.215994	381263.907227	46.340365
3237.685050	377671.039173	46.345370
3233.668057	374072.813160	46.350375
3229.688175	370480.901048	46.355380
3225.915105	366877.638757	46.360385
3221.852852	363282.776793	46.365389
3217.814111	359690.071016	46.370394
3213.878295	356112.926478	46.375399
3209.807702	352526.593154	46.380404
3206.156803	348941.191212	46.385409
3202.085471	345378.905876	46.390413
3198.117462	341809.080537	46.395418
3194.045359	338232.140646	46.400423
3190.170416	334666.701222	46.405428
3186.136978	331110.620116	46.410433
3182.028507	327562.852859	46.415437
3178.411500	324001.580127	46.420442
3174.665390	320449.747238	46.425447
3170.137585	316910.223788	46.430452
3166.482270	313359.174936	46.435457
3162.514696	309834.588004	46.440461
3158.373286	306307.658037	46.445466
3154.585583	302795.419047	46.450471
3150.278198	299286.645437	46.455476
3146.465007	295773.898304	46.460481
3142.254670	292282.010130	46.465485
3138.112975	288789.652839	46.470490
3134.381671	285296.169283	46.475495
3129.706324	281837.369940	46.480500
3126.040321	278364.532227	46.485505
3121.850577	274912.706921	46.490509
3118.083652	271461.680386	46.495514
3114.098709	268028.937546	46.500519
3109.831994	264595.067126	46.505524
3106.071873	261167.971501	46.510529
3101.866636	257773.565959	46.515533
3098.072115	254361.903165	46.520538
3094.055595	250951.663513	46.525543
3089.763367	247559.979982	46.530548
3086.185933	244170.933870	46.535553
3081.913252	240796.303837	46.540557
3078.123877	237440.615745	46.545562
3074.083348	234070.536140	46.550567
3070.055952	230721.862136	46.555572
3066.255838	227367.522091	46.560577
3062.108960	224040.062241	46.565581
3058.195107	220710.263171	46.570586
3054.094443	217387.573768	46.575591
3049.720028	214078.815080	46.580596
3045.977909	210778.931100	46.585601
3042.041766	207492.865166	46.590605
3037.820004	204182.616188	46.595610
3033.991790	200858.203695	46.600615
3029.807682	197597.239949	46.605620
3026.097867	194339.601583	46.610625
3021.883130	191106.941427	46.615629
3017.745691	187870.991595	46.620634
3014.058101	184650.609878	46.625639
3009.699457	181444.192476	46.630644
3006.005775	178228.392179	46.635649
3001.767055	175035.697560	46.640653
2997.982155	171851.660113	46.645658
2993.951545	168670.753033	46.650663
2989.832749	165518.551736	46.655668
2985.865326	162367.200161	46.660673
2981.490830	159225.166952	46.665677
2977.644204	156093.626135	46.670682
2973.406252	152974.883611	46.675687
2969.640007	149879.482793	46.680692
2965.886624	146778.511342	46.685697
2961.887091	143695.401201	46.690701
2957.684625	140615.096267	46.695706
2953.418929	137548.321162	46.700711
2949.302453	134507.220787	46.705716
2945.422398	131460.745164	46.710721
2941.159367	128439.427580	46.715725
2937.280590	125420.993538	46.720730
2933.103395	122423.311014	46.725735
2929.036504	119429.442148	46.730740
2925.117622	116448.710083	46.735745
2920.975824	113489.269376	46.740749
2917.163255	110537.325378	46.745754
2912.906022	107602.876685	46.750759
2908.832647	104677.770210	46.755764
2904.709800	101750.557833	46.760769
2900.470883	98858.135000	46.765773
2896.131749	95977.956943	46.770778
2892.231368	93098.311104	46.775783
2887.962610	90257.336850	46.780788
2883.924368	87415.713581	46.785793
2879.798795	84591.014209	46.790797
2875.812103	81789.778462	46.795802
2871.633930	78991.072254	46.800807
2867.309567	76231.563871	46.805812
2863.268712	73462.047783	46.810817
2859.252828	70718.153610	46.815821
2854.727926	67996.320187	46.820826
2850.561893	65285.246231	46.825831
2846.035224	62598.695268	46.830836
2841.886978	59918.412564	46.835841
2837.343627	57272.195334	46.840845
2832.882292	54652.082258	46.845850
2828.341366	52050.227688	46.850855
2823.586029	49477.505931	46.855860
2819.417220	46926.283552	46.860865
2814.273748	44406.086020	46.865869
2809.697170	41925.260292	46.870874
2804.150643	39483.712733	46.875879
2796.939573	37129.806798	46.880884
2788.424010	34860.769717	46.885889
2779.616098	32677.664883	46.890893
2771.458442	30571.185271	46.895898
2763.442731	28566.411635	46.900903
2755.515146	26651.182302	46.905908
2748.205356	24832.234775	46.910913
2740.693114	23111.389341	46.915917
2733.419382	21485.170077	46.920922
2726.565759	19949.232723	46.925927
2719.643892	18508.258840	46.930932
2713.582184	17147.133698	46.935937
2707.454947	15871.397297	46.940941
2701.604065	14671.921368	46.945946
2695.720228	13544.958156	46.950951
2689.475974	12505.074837	46.955956
2683.783065	11519.343149	46.960961
2677.465513	10622.721425	46.965965
2671.473791	9785.874832	46.970970
2665.391296	9007.570079	46.975975
2659.958630	8314.280046	46.980980
2654.306782	7672.059097	46.985985
2648.824732	7090.813400	46.990989
2643.728137	6552.455665	46.995994
2639.182865	6064.344643	47.000999
2634.449202	5620.335971	47.006004
2630.181150	5202.918018	47.011009
2626.361118	4831.553632	47.016013
2622.383611	4471.601834	47.021018
2618.641864	4150.085346	47.026023
2615.374442	3841.899752	47.031028
2611.676601	3540.700450	47.036033
2608.616682	3263.042650	47.041037
2605.062198	2982.126246	47.046042
2602.240918	2709.839092	47.051047
2598.341861	2460.463275	47.056052
2595.713270	2200.546064	47.061057
2592.219640	1958.215782	47.066061
2589.313514	1709.478349	47.071066
2586.119875	1480.653618	47.076071
2582.889616	1241.566376	47.081076
2580.022294	997.028901	47.086081
2576.444034	770.869328	47.091085
2572.913799	544.213740	47.096090
2569.234259	324.658886	47.101095
2564.574713	140.988113	47.106100
2552.933884	160.250958	47.111105
2543.929034	172.470626	47.116109
2538.883599	170.599476	47.121114
2536.474111	170.104668	47.126119
2534.776873	180.660037	47.131124
2532.995166	163.100746	47.136129
2530.740559	170.171099	47.141133
2528.123040	167.370562	47.146138
2525.409418	155.499129	47.151143
2521.976592	165.742414	47.156148
2518.296455	154.688248	47.161153
2515.191198	165.977646	47.166157
2511.608450	170.232115	47.171162
2508.725587	162.435889	47.176167
2505.344121	157.560515	47.181172
2502.293540	159.917537	47.186177
2499.037574	157.140499	47.191181
2495.432733	162.101749	47.196186
2492.276216	155.751233	47.201191
2488.180697	156.605314	47.206196
2485.084863	142.854383	47.211201
2481.864313	151.612586	47.216205
2478.213481	161.033247	47.221210
2475.564674	148.473290	47.226215
2471.637952	162.987469	47.231220
2468.666172	161.753321	47.236225
2465.282071	160.172226	47.241229
2461.882736	165.395589	47.246234
2458.663810	150.575471	47.251239
2454.438377	157.581213	47.256244
2451.312428	150.757985	47.261249
2447.726668	155.569689	47.266253
2444.497092	154.982367	47.271258
2441.905728	151.708484	47.276263
2437.456901	159.828989	47.281268
2433.776793	157.056491	47.286273
2430.558724	160.054142	47.291277
2427.450827	158.315984	47.296282
2424.194287	153.174755	47.301287
2420.295087	154.494769	47.306292
2417.288829	158.925284	47.311297
2414.290338	158.223268	47.316301
2410.494837	153.324547	47.321306
2406.901552	152.807155	47.326311
2403.134542	159.965587	47.331316
2400.022148	151.711215	47.336321
2396.330583	154.199368	47.341325
2392.780546	149.554575	47.346330
2389.675005	148.429190	47.351335
2385.865354	147.819654	47.356340
2382.502584	146.132283	47.361345
2379.427349	150.127425	47.366349
2375.852224	153.199444	47.371354
2372.570327	145.954844	47.376359
2368.910246	146.177285	47.381364
2365.331698	149.556148	47.386369
2361.807388	146.985720	47.391373
2358.061369	144.756982	47.396378
2354.913345	141.002759	47.401383
2351.452480	149.655661	47.406388
2347.820325	149.161700	47.411393
2344.647234	146.316032	47.416397
2340.773177	150.574302	47.421402
2337.542828	143.889362	47.426407
2333.790339	147.905560	47.431412
2330.574438	139.915796	47.436417
2327.396484	139.453629	47.441421
2323.533040	143.715881	47.446426
2320.217347	139.022593	47.451431
2316.471893	140.592595	47.456436
2313.203760	148.229762	47.461441
2309.470224	146.689891	47.466445
2305.880707	147.348297	47.471450
2303.016272	151.125155	47.476455
2299.351759	151.286217	47.481460
2295.700800	153.201768	47.486465
2292.538430	141.921030	47.491469
2288.729923	143.607237	47.496474
2285.690441	141.163240	47.501479
2281.718194	145.867965	47.506484
2278.336647	145.984102	47.511489
2275.006951	146.554443	47.516493
2271.030640	151.202423	47.521498
2267.778160	147.731518	47.526503
2264.055565	141.747552	47.531508
2260.563541	148.012312	47.536513
2257.666954	149.263418	47.541517
2254.229775	153.548688	47.546522
2250.419449	150.749090	47.551527
2246.974496	150.908278	47.556532
2243.551066	149.793834	47.561537
2240.132061	146.843596	47.566541
2236.314734	152.092302	47.571546
2232.941371	137.809187	47.576551
2229.215131	143.009704	47.581556
2226.017784	144.667278	47.586561
2222.913910	145.267859	47.591565
2218.932929	151.461427	47.596570
2215.461484	143.111367	47.601575
2212.106968	151.742059	47.606580
2208.605340	142.788589	47.611585
2205.128249	146.358609	47.616589
2201.706083	146.105573	47.621594
2198.530883	142.913429	47.626599
2194.830216	149.888375	47.631604
2190.995156	144.808108	47.636609
2187.739238	132.388268	47.641613
2184.234846	139.399285	47.646618
2180.693791	138.787989	47.651623
2177.070747	147.619135	47.656628
2173.773606	136.539931	47.661633
2170.478305	131.579544	47.666637
2166.980926	136.340134	47.671642
2163.347610	136.462797	47.676647
2159.482348	148.593018	47.681652
2155.875686	140.706981	47.686657
2152.640036	137.297714	47.691661
2149.312752	148.720645	47.696666
2145.796922	140.216942	47.701671
2142.012425	145.835832	47.706676
2138.668485	143.914636	47.711681
2135.527558	128.920500	47.716685
2132.039518	140.703090	47.721690
2128.173857	140.386584	47.726695
2124.532381	137.475143	47.731700
2121.000692	135.468139	47.736705
2118.092271	139.239730	47.741709
2114.222032	132.344093	47.746714
2111.139561	133.777733	47.751719
2107.068696	136.087187	47.756724
2103.818174	130.614265	47.761729
2100.106429	133.073798	47.766733
2096.579257	132.163671	47.771738
2093.234299	130.147955	47.776743
2089.855370	140.272265	47.781748
2086.282550	137.979622	47.786753
2083.108148	132.956511	47.791757
2079.151388	134.009627	47.796762
2076.331206	127.256758	47.801767
2072.422033	138.984210	47.806772
2068.898190	134.673391	47.811777
2065.398747	139.543521	47.816781
2061.549346	137.867870	47.821786
2058.110150	138.218253	47.826791
2054.522976	141.780703	47.831796
2051.434135	130.269562	47.836801
2047.785412	125.979189	47.841805
2044.372475	132.769563	47.846810
2041.271154	126.356196	47.851815
2037.508779	137.323351	47.856820
2033.906388	127.357154	47.861825
2030.408904	129.406605	47.866829
2026.753579	132.834298	47.871834
2023.326080	125.329454	47.876839
2019.788537	126.291676	47.881844
2016.462720	131.683542	47.886849
2012.457384	126.033616	47.891853
2009.127644	125.605411	47.896858
2005.546819	126.032899	47.901863
2002.394559	133.280898	47.906868
1999.024360	134.774955	47.911873
1995.400819	133.577113	47.916877
1992.071216	135.303844	47.921882
1988.682403	126.854288	47.926887
1984.990355	132.370400	47.931892
1981.245718	135.441879	47.936897
1977.694240	130.973088	47.941901
1974.151279	138.109016	47.946906
1971.267500	133.113368	47.951911
1967.907637	134.230401	47.956916
1964.014531	132.984553	47.961921
1960.199151	127.192198	47.966925
1956.850751	131.084303	47.971930
1953.391521	130.343428	47.976935
1949.541994	128.440754	47.981940
1946.277822	132.233309	47.986945
1943.201395	120.084579	47.991949
1939.325895	123.049628	47.996954
1935.976424	119.076576	48.001959
1932.576652	127.415339	48.006964
1928.966515	126.704144	48.011969
1925.351419	124.563062	48.016973
1921.428338	131.755097	48.021978
1918.415133	123.898726	48.026983
1915.138966	128.298718	48.031988
1911.587273	131.632414	48.036993
1908.274292	120.838444	48.041997
1904.308954	129.044689	48.047002
1900.838475	123.369273	48.052007
1897.127439	133.627881	48.057012
1893.924417	125.682108	48.062017
1890.512343	117.639446	48.067021
1886.585383	121.508363	48.072026
1883.261591	117.718778	48.077031
1879.841210	123.773422	48.082036
1876.236712	119.109031	48.087041
1873.269400	119.674451	48.092045
1869.215207	123.063750	48.097050
1866.301243	120.973454	48.102055
1862.627980	121.714496	48.107060
1859.131181	122.921910	48.112065
1855.528742	125.807977	48.117069
1851.375727	127.983798	48.122074
1848.506171	125.240681	48.127079
1844.917054	122.650964	48.132084
1841.547111	125.359117	48.137089
1838.071483	127.388124	48.142093
1834.254076	121.193643	48.147098
1830.941148	121.432752	48.152103
1827.364873	119.425840	48.157108
1823.930809	126.484475	48.162113
1820.203849	115.680228	48.167117
1816.635447	123.166786	48.172122
1813.450722	117.307481	48.177127
1809.986033	122.198285	48.182132
1806.351779	116.082703	48.187137
1802.850584	121.602343	48.192141
1799.506011	121.120297	48.197146
1796.106832	119.799902	48.202151
1792.309186	115.352394	48.207156
1788.685809	122.594078	48.212161
1785.447254	121.547504	48.217165
1781.792551	120.157046	48.222170
1778.179480	115.209984	48.227175
1774.627196	125.970522	48.232180
1771.124356	120.184521	48.237185
1767.822917	111.922990	48.242189
1764.677078	117.736395	48.247194
1761.007524	118.701869	48.252199
1757.479141	122.730204	48.257204
1753.974482	120.020043	48.262209
1750.758817	122.169757	48.267213
1746.655438	125.505318	48.272218
1743.406490	120.834392	48.277223
1739.503025	124.829787	48.282228
1736.070353	117.726038	48.287233
1733.315037	120.341207	48.292237
1729.569262	124.602422	48.297242
1725.724974	120.848821	48.302247
1722.296946	115.633638	48.307252
1718.786249	123.036332	48.312257
1715.556236	109.145995	48.317261
1711.457034	118.628977	48.322266
1708.486702	113.958224	48.327271
1704.696341	118.814694	48.332276
1701.346724	117.579126	48.337281
1698.289574	111.932875	48.342285
1694.361867	123.693242	48.347290
1690.930905	115.493031	48.352295
1687.508066	118.059853	48.357300
1684.263449	123.384245	48.362305
1680.613752	114.851357	48.367309
1676.380814	126.350375	48.372314
1673.130238	117.346610	48.377319
1669.099144	123.790806	48.382324
1665.841348	122.467472	48.387329
1662.760515	114.716398	48.392333
1659.360855	123.947677	48.397338
1656.063210	115.980626	48.402343
1652.496657	126.757413	48.407348
1649.172089	122.639758	48.412353
1645.516035	116.694862	48.417357
1641.246181	121.303223	48.422362
1638.350388	113.703933	48.427367
1634.878862	114.713746	48.432372
1631.657290	115.515707	48.437377
1628.003279	111.666421	48.442381
1624.332754	115.484884	48.447386
1620.521864	118.878586	48.452391
1617.124637	115.953047	48.457396
1613.560394	117.566264	48.462401
1610.673117	111.199348	48.467405
1606.732996	109.733842	48.472410
1603.217821	112.680069	48.477415
1599.804849	117.687779	48.482420
1596.294119	111.762919	48.487425
1592.901139	114.560298	48.492429
1588.846558	122.435985	48.497434
1585.721642	107.037501	48.502439
1582.197084	116.589417	48.507444
1579.048460	114.543213	48.512449
1575.458371	112.251458	48.517453
1571.493922	121.180455	48.522458
1568.268995	115.921372	48.527463
1564.556715	111.366417	48.532468
1561.121354	109.763666	48.537473
1557.614752	115.729758	48.542477
1554.520325	116.192257	48.547482
1551.027174	107.090149	48.552487
1547.389460	117.767459	48.557492
1543.525639	100.128984	48.562497
1540.565544	108.341651	48.567501
1536.345067	112.045039	48.572506
1533.168123	104.285085	48.577511
1529.545314	114.526193	48.582516
1526.222969	108.406075	48.587521
1522.990411	105.889514	48.592525
1518.872285	112.177314	48.597530
1516.017484	104.956940	48.602535
1512.003079	109.794930	48.607540
1508.407085	114.708229	48.612545
1505.413133	110.455141	48.617549
1501.773366	122.157996	48.622554
1498.545284	103.563774	48.627559
1494.588694	114.530227	48.632564
1490.755078	111.352085	48.637569
1488.106373	115.194383	48.642573
1484.315620	111.883656	48.647578
1480.681815	112.251425	48.652583
1476.749925	110.844267	48.657588
1473.748852	110.816991	48.662593
1470.153644	103.235930	48.667597
1466.525944	111.306775	48.672602
1462.967933	106.699574	48.677607
1459.858387	112.163007	48.682612
1456.782564	118.632624	48.687617
1452.889497	111.853054	48.692621
1448.849925	105.565000	48.697626
1446.066985	108.510502	48.702631
1442.020758	110.561674	48.707636
1438.597786	112.640677	48.712641
1435.077222	104.102455	48.717645
1431.557926	102.690886	48.722650
1428.320073	109.950402	48.727655
1424.832134	108.445247	48.732660
1421.049526	110.513252	48.737665
1417.740572	99.568467	48.742669
1413.815639	110.883176	48.747674
1410.651290	106.313569	48.752679
1407.036284	115.324056	48.757684
1403.393949	118.599688	48.762689
1400.255884	101.954389	48.767693
1396.390780	115.880069	48.772698
1393.047364	109.500684	48.777703
1389.635900	112.262582	48.782708
1386.404658	109.755770	48.787713
1382.713519	105.842573	48.792717
1378.812529	113.283757	48.797722
1375.727927	103.968242	48.802727
1371.964199	113.021094	48.807732
1368.046424	123.451181	48.812737
1364.969908	110.257432	48.817741
1361.549357	116.597996	48.822746
1358.172370	107.492440	48.827751
1355.034377	119.641711	48.832756
1350.874399	113.654855	48.837761
1347.987538	117.070482	48.842765
1343.916077	114.534056	48.847770
1340.522071	118.185861	48.852775
1337.275089	109.290902	48.857780
1333.775356	109.112693	48.862785
1330.144367	108.269053	48.867789
1326.336731	115.387394	48.872794
1323.118641	112.631189	48.877799
1319.447864	114.819519	48.882804
1315.837675	114.384296	48.887809
1312.557100	96.750688	48.892813
1309.028699	95.564304	48.897818
1305.852940	95.892804	48.902823
1302.092701	106.536850	48.907828
1298.293718	107.402125	48.912833
1294.769953	104.849212	48.917837
1291.309482	113.828115	48.922842
1287.739240	111.693153	48.927847
1284.576012	112.043277	48.932852
1281.101221	119.103475	48.937857
1277.895485	107.953083	48.942861
1274.132685	113.702225	48.947866
1270.562947	108.182263	48.952871
1267.048180	110.771882	48.957876
1263.002198	112.015662	48.962881
1260.325826	103.343759	48.967885
1256.797867	111.251444	48.972890
1253.316468	105.391484	48.977895
1249.211946	102.100863	48.982900
1245.822860	105.352113	48.987905
1242.490714	103.806348	48.992909
1238.744830	116.600630	48.997914
1235.663240	105.641692	49.002919
1231.996089	108.744149	49.007924
1228.445503	113.869388	49.012929
1225.199832	99.944175	49.017933
1221.107224	115.072469	49.022938
1217.706143	106.315567	49.027943
1214.611037	112.843572	49.032948
1211.101131	111.337874	49.037953
1207.728772	105.625885	49.042957
1203.780933	111.651949	49.047962
1200.232807	104.238771	49.052967
1197.138987	107.665021	49.057972
1193.543133	108.308737	49.062977
1190.141073	104.807906	49.067981
1186.023446	107.473968	49.072986
1182.732926	102.077038	49.077991
1179.462703	105.207646	49.082996
1175.942262	110.490347	49.088001
1172.725201	98.917054	49.093005
1168.924667	101.294690	49.098010
1165.584694	101.706284	49.103015
1161.947047	102.992755	49.108020
1158.438455	100.659053	49.113025
1155.222985	93.187960	49.118029
1151.350794	109.443949	49.123034
1147.874589	101.638855	49.128039
1144.506276	102.385098	49.133044
1140.779808	101.169630	49.138049
1137.363873	108.145993	49.143053
1133.421196	103.473212	49.148058
1130.363099	103.996688	49.153063
1126.936991	99.096817	49.158068
1123.317151	105.564027	49.163073
1120.271155	98.069871	49.168077
1116.151359	104.530752	49.173082
1113.008586	103.815544	49.178087
1109.651450	104.629428	49.183092
1105.851872	108.476528	49.188097
1102.531782	90.684678	49.193101
1098.630017	98.542976	49.198106
1095.317188	100.276042	49.203111
1091.612518	105.632283	49.208116
1088.363010	108.131998	49.213121
1085.115724	97.301226	49.218125
1081.400222	104.272101	49.223130
1077.758727	100.235121	49.228135
1074.309174	105.531826	49.233140
1070.646353	104.351872	49.238145
1067.496015	101.600442	49.243149
1063.879956	110.759540	49.248154
1060.458899	103.923403	49.253159
1056.886187	105.274800	49.258164
1053.082410	99.578431	49.263169
1049.606943	98.547683	49.268173
1045.890876	106.128648	49.273178
1042.824909	96.731776	49.278183
1039.469789	93.440967	49.283188
1035.850177	99.276526	49.288193
1032.363408	96.344544	49.293197
1028.758721	97.634550	49.298202
1025.207770	96.084284	49.303207
1021.768716	99.556882	49.308212
1018.041435	105.152144	49.313217
1015.195311	95.487069	49.318221
1011.089550	105.102713	49.323226
1007.644636	91.341085	49.328231
1004.204548	111.203290	49.333236
1000.645730	111.304474	49.338241
997.067503	105.148948	49.343245
994.016429	98.421000	49.348250
990.445812	104.007544	49.353255
987.000393	102.309613	49.358260
983.250801	96.597244	49.363265
980.093065	94.944492	49.368269
975.899308	103.043778	49.373274
972.622528	97.424120	49.378279
969.021563	97.002253	49.383284
965.416450	106.271103	49.388289
962.472132	100.156014	49.393293
958.810033	110.218512	49.398298
955.310243	102.145750	49.403303
951.538521	101.809365	49.408308
948.005897	110.111723	49.413313
944.924264	104.919408	49.418317
941.295652	105.374759	49.423322
937.741228	92.133134	49.428327
934.245108	91.827948	49.433332
930.562498	99.700652	49.438337
927.190298	98.027759	49.443341
923.752475	102.835209	49.448346
920.260818	99.318824	49.453351
916.819243	96.035108	49.458356
912.916795	107.726934	49.463361
909.927854	99.122560	49.468365
906.180858	107.538348	49.473370
902.643998	104.106612	49.478375
899.237500	101.219674	49.483380
895.629779	101.567808	49.488385
892.207453	100.694947	49.493389
888.710534	112.523967	49.498394
884.943905	105.417553	49.503399
881.695810	102.751101	49.508404
878.296840	108.991927	49.513409
874.931642	95.489952	49.518413
871.066659	99.208935	49.523418
868.051724	104.797791	49.528423
864.436732	94.959059	49.533428
860.420488	96.882048	49.538433
857.182003	103.793533	49.543437
853.363350	93.002802	49.548442
849.908729	96.200843	49.553447
846.598822	90.504280	49.558452
842.944665	104.532795	49.563457
839.899269	92.591382	49.568461
835.979898	99.969918	49.573466
832.510017	102.071530	49.578471
828.935641	92.992964	49.583476
825.335502	95.274982	49.588481
822.280476	95.175167	49.593485
818.884111	101.933018	49.598490
815.299763	97.623170	49.603495
811.716980	97.797932	49.608500
807.822395	98.199902	49.613505
804.396876	92.543810	49.618509
801.056577	101.592946	49.623514
797.687494	92.523864	49.628519
794.161172	99.067410	49.633524
790.557818	89.151641	49.638529
786.990944	89.268932	49.643533
783.311185	85.510666	49.648538
780.158149	87.292711	49.653543
776.567226	87.237570	49.658548
773.019676	92.225290	49.663553
769.705939	87.941760	49.668557
766.212187	99.128787	49.673562
762.795558	90.062076	49.678567
759.017859	83.906611	49.683572
755.226855	90.165403	49.688577
751.756142	87.591331	49.693581
748.679891	89.319452	49.698586
744.874096	84.133622	49.703591
741.560234	90.155623	49.708596
737.929576	97.081542	49.713601
734.579507	85.922936	49.718605
730.983560	92.164082	49.723610
727.933097	92.773003	49.728615
724.219432	91.699629	49.733620
720.537612	87.439143	49.738625
716.609829	88.718320	49.743629
712.956992	87.815653	49.748634
709.922821	84.117004	49.753639
706.839206	83.508729	49.758644
703.188922	92.047391	49.763649
699.722424	82.402113	49.768653
696.076119	94.766469	49.773658
692.575294	92.568616	49.778663
688.950858	89.997333	49.783668
685.430163	86.185604	49.788673
681.891558	84.262388	49.793677
678.371943	96.360115	49.798682
674.795978	88.032819	49.803687
671.907152	92.985438	49.808692
668.052974	83.562393	49.813697
664.577238	89.129925	49.818701
660.599280	95.644687	49.823706
657.460862	94.665247	49.828711
654.228137	90.969096	49.833716
650.190544	87.915043	49.838721
646.691190	77.338695	49.843725
643.283230	94.453193	49.848730
639.905654	86.810423	49.853735
636.616001	83.064704	49.858740
632.894543	87.751355	49.863745
629.738580	84.109817	49.868749
625.628873	94.919124	49.873754
622.336146	93.190301	49.878759
618.883724	99.141778	49.883764
615.505796	95.956312	49.888769
611.975684	86.198103	49.893773
608.190987	100.873138	49.898778
604.682973	96.836387	49.903783
601.446120	91.412495	49.908788
597.869049	96.613225	49.913793
594.344637	92.234056	49.918797
590.863103	93.088644	49.923802
587.319591	95.248802	49.928807
583.836802	91.480615	49.933812
580.336589	92.566817	49.938817
577.417457	88.385292	49.943821
573.280657	93.193998	49.948826
570.058354	89.063234	49.953831
566.618489	97.119625	49.958836
562.792642	102.183748	49.963841
559.345146	87.220402	49.968845
555.647934	97.276758	49.973850
552.038563	87.734974	49.978855
548.722882	88.576162	49.983860
545.287387	93.535448	49.988865
541.757737	89.245401	49.993869
537.941469	81.906590	49.998874
534.733991	90.617392	50.003879
531.692975	93.168642	50.008884
528.069388	89.565882	50.013889
524.694762	84.689371	50.018893
521.160132	92.104739	50.023898
516.785468	95.234458	50.028903
513.663973	89.212368	50.033908
509.936800	84.250350	50.038913
507.228745	84.928859	50.043917
503.310920	93.138978	50.048922
499.703118	81.427084	50.053927
496.259825	82.036247	50.058932
492.559912	84.909089	50.063937
489.089798	82.446827	50.068941
485.890479	87.374570	50.073946
482.510438	87.136772	50.078951
479.181369	80.137718	50.083956
475.201581	90.542420	50.088961
472.075961	75.876765	50.093965
468.265793	99.924815	50.098970
464.541136	86.377727	50.103975
460.932841	90.900354	50.108980
457.437576	101.702249	50.113985
454.118034	87.089017	50.118989
450.509423	90.335733	50.123994
446.967047	87.415410	50.128999
443.759423	85.749209	50.134004
440.159739	92.143537	50.139009
437.243186	87.466571	50.144013
433.350192	94.421137	50.149018
429.737697	86.100111	50.154023
426.294044	93.045241	50.159028
422.543144	94.030778	50.164033
419.367339	84.098668	50.169037
415.579143	91.508522	50.174042
412.108355	89.359802	50.179047
408.671347	91.254227	50.184052
405.258544	102.722529	50.189057
401.972670	85.563276	50.194061
398.108555	93.700853	50.199066
394.481703	93.190603	50.204071
391.035706	90.651020	50.209076
387.566564	98.290876	50.214081
384.672271	90.389747	50.219085
380.817241	92.877109	50.224090
377.289880	94.200624	50.229095
373.710680	85.749818	50.234100
370.111866	98.158643	50.239105
366.485317	80.459073	50.244109
363.053141	84.897174	50.249114
359.501937	86.855333	50.254119
356.256377	80.736885	50.259124
352.974803	83.786480	50.264129
349.404477	88.284360	50.269133
345.582514	87.191352	50.274138
341.846324	88.083749	50.279143
338.642980	81.610227	50.284148
335.070219	86.402156	50.289153
331.610947	74.543497	50.294157
327.712194	88.860098	50.299162
324.711654	79.310308	50.304167
321.092033	85.074381	50.309172
317.657245	83.948293	50.314177
314.597000	79.131021	50.319181
310.841369	89.840142	50.324186
307.164126	90.475354	50.329191
303.478698	79.289965	50.334196
299.949685	90.157538	50.339201
296.625181	81.415609	50.344205
292.877549	92.127961	50.349210
289.829610	87.905804	50.354215
286.463324	81.604141	50.359220
282.549816	88.921574	50.364225
279.028308	82.341912	50.369229
275.380209	84.517263	50.374234
271.921663	82.187454	50.379239
268.684898	73.891216	50.384244
264.706227	84.176119	50.389249
261.800439	79.695034	50.394253
258.243179	78.944275	50.399258
254.496488	90.455902	50.404263
251.147156	78.405263	50.409268
247.283162	82.832251	50.414273
244.045965	75.896335	50.419277
240.456523	81.404266	50.424282
237.010278	75.587516	50.429287
233.623454	86.767853	50.434292
229.607002	88.299735	50.439297
226.528772	79.656615	50.444301
223.119043	83.919622	50.449306
219.811509	73.490307	50.454311
216.144494	78.705230	50.459316
212.316323	76.941445	50.464321
208.561264	76.241036	50.469325
205.164157	74.084043	50.474330
202.102881	85.870789	50.479335
198.926778	82.561283	50.484340
195.234482	88.669207	50.489345
191.484581	85.841477	50.494349
188.046895	86.792728	50.499354
184.491102	82.775499	50.504359
180.908189	83.957803	50.509364
177.238486	87.304048	50.514369
174.036157	78.507468	50.519373
170.569640	83.831711	50.524378
166.948742	81.727783	50.529383
163.204069	83.118233	50.534388
159.676944	79.967514	50.539393
156.388942	85.001731	50.544397
152.678584	77.947484	50.549402
149.357371	78.790287	50.554407
146.131328	82.718452	50.559412
142.352990	85.893665	50.564417
139.353918	81.758847	50.569421
135.652054	80.792766	50.574426
132.025363	78.509069	50.579431
128.738434	82.884029	50.584436
124.876251	82.829744	50.589441
121.647497	74.449424	50.594445
118.080030	78.056834	50.599450
114.094551	72.756703	50.604455
110.823904	75.377634	50.609460
106.770562	77.828212	50.614465
103.924307	73.578728	50.619469
100.284382	81.012432	50.624474
97.172028	83.301493	50.629479
93.796955	80.062113	50.634484
90.042632	83.310355	50.639489
86.597985	77.908268	50.644493
82.910749	82.100507	50.649498
79.353503	78.005074	50.654503
75.874444	83.811383	50.659508
71.871559	86.069725	50.664513
69.098543	79.675540	50.669517
65.466184	83.967242	50.674522
61.697438	75.634354	50.679527
58.407903	81.050539	50.684532
54.864380	86.520625	50.689537
51.361636	85.159339	50.694541
47.863226	88.533766	50.699546
44.116563	89.382374	50.704551
40.787546	80.948273	50.709556
37.550283	82.442279	50.714561
34.234972	81.255594	50.719565
30.497633	88.736271	50.724570
26.657818	93.175432	50.729575
22.944802	84.199114	50.734580
19.432468	84.775099	50.739585
16.342409	78.383331	50.744589
12.893878	90.239648	50.749594
9.396545	75.435073	50.754599
6.079235	78.270814	50.759604
2.230596	91.799502	50.764609