Tue Jun 21 10:43:27 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.012493	113.217978	0.000000
0.482864	111.510204	0.005005
0.708168	102.821612	0.010010
0.486197	94.885532	0.015014
0.421299	97.937072	0.020019
0.667096	88.879433	0.025024
0.408933	87.838492	0.030029
0.159308	73.542575	0.035034
0.004225	72.929158	0.040038
-0.525745	58.959303	0.045043
-0.675493	46.428403	0.050048
-1.015148	40.381577	0.055053
-1.405644	26.990720	0.060058
-1.661535	22.831141	0.065062
-2.026676	12.894368	0.070067
-1.870710	10.179346	0.075072
-2.411991	-1.025913	0.080077
-2.664866	-6.876339	0.085082
-3.192211	-9.150428	0.090086
-3.117603	-2.377219	0.095091
-4.001505	-8.054274	0.100096
-4.755214	0.587708	0.105101
-4.881325	-9.079020	0.110106
-4.979570	-2.798737	0.115110
-4.862478	-10.857612	0.120115
-4.949983	-5.509929	0.125120
-5.399092	-4.865985	0.130125
-5.264110	0.239825	0.135130
-5.304059	-1.269012	0.140134
-6.223216	1.742432	0.145139
-6.504694	-4.544297	0.150144
-6.942009	0.608140	0.155149
-6.819486	-6.092603	0.160154
-6.848499	-4.355936	0.165158
-7.679557	2.291386	0.170163
-7.135911	-9.675669	0.175168
-8.259658	-2.835035	0.180173
-8.095321	-7.695268	0.185178
-8.522352	-3.096476	0.190182
-8.688217	3.370436	0.195187
-8.577690	-2.094594	0.200192
-8.833669	5.401733	0.205197
-9.230280	-0.613739	0.210202
-9.615861	0.948927	0.215206
-9.915351	-2.008965	0.220211
-9.651782	-4.137767	0.225216
-10.056602	-0.908791	0.230221
-11.184902	1.994421	0.235226
-11.428426	-4.901052	0.240230
-11.425642	-5.638486	0.245235
-11.504368	2.393252	0.250240
-11.793093	5.181500	0.255245
-11.419629	2.085522	0.260250
-11.399419	-0.127102	0.265254
-11.888823	-2.959809	0.270259
-12.405115	-2.123784	0.275264
-12.783188	3.095408	0.280269
-13.014336	-1.773331	0.285274
-12.756243	7.582187	0.290278
-13.957488	7.262792	0.295283
-14.258241	-3.676428	0.300288
-14.646661	6.680075	0.305293
-14.530516	2.283660	0.310298
-14.363061	3.555237	0.315302
-14.574695	-1.796057	0.320307
-14.565894	3.690389	0.325312
-15.261828	7.956415	0.330317
-15.786843	-4.819937	0.335322
-16.062860	-6.573444	0.340326
-16.454628	1.831000	0.345331
-15.981857	-6.016631	0.350336
-16.482793	-0.624555	0.355341
-17.210468	0.613518	0.360346
-17.594924	-10.686176	0.365350
-17.857423	0.957394	0.370355
-17.734689	-9.271897	0.375360
-17.677454	-0.791248	0.380365
-17.636439	-1.931062	0.385370
-17.811455	-5.553070	0.390374
-18.708827	2.262989	0.395379
-19.080389	-7.154705	0.400384
-19.386057	-5.521011	0.405389
-19.443355	-10.137931	0.410394
-19.622920	-7.823010	0.415398
-19.595598	-3.875083	0.420403
-19.947615	-16.060843	0.425408
-20.746792	-3.613264	0.430413
-20.972322	-4.835228	0.435418
-20.831246	-4.827741	0.440422
-21.056243	-8.455285	0.445427
-21.079023	-14.240409	0.450432
-21.145180	-7.990110	0.455437
-22.127538	-3.360918	0.460442
-22.270892	-12.446402	0.465446
-22.467866	-12.191518	0.470451
-22.791953	-14.916624	0.475456
-22.866050	-2.706734	0.480461
-22.897602	-9.901339	0.485466
-22.957942	-7.031134	0.490470
-23.989077	4.729075	0.495475
-24.243007	-14.492861	0.500480
-24.489968	-0.491763	0.505485
-24.569646	-9.864454	0.510490
-24.194192	-1.635813	0.515494
-24.410457	-0.272076	0.520499
-25.075991	-4.296513	0.525504
-25.764121	4.508462	0.530509
-25.896748	-0.693510	0.535514
-25.613315	1.555984	0.540518
-25.938400	-7.956430	0.545523
-26.023643	-1.865570	0.550528
-27.089014	-4.992030	0.555533
-27.490661	-0.435723	0.560538
-27.689191	-2.927459	0.565542
-27.572226	3.245552	0.570547
-27.536453	-9.128359	0.575552
-27.879066	4.088596	0.580557
-27.825813	-0.578405	0.585562
-27.698419	-6.373405	0.590566
-28.798450	-1.067604	0.595571
-28.657894	-12.106739	0.600576
-29.134771	-0.610990	0.605581
-29.197917	-3.392139	0.610586
-29.944625	-1.034796	0.615590
-30.398279	2.443411	0.620595
-30.534055	-8.526677	0.625600
-30.502847	-0.243393	0.630605
-30.502003	-2.515166	0.635610
-30.319445	0.454525	0.640614
-30.721156	2.563123	0.645619
-31.191966	-1.833764	0.650624
-31.723106	-3.336043	0.655629
-32.112180	-4.392395	0.660634
-32.140709	3.968272	0.665638
-32.404205	-5.212757	0.670643
-32.201231	-6.335980	0.675648
-33.229359	3.189329	0.680653
-33.434248	1.075553	0.685658
-33.402187	-9.509904	0.690662
-33.967329	1.532193	0.695667
-33.605003	-6.489349	0.700672
-34.048754	-8.415764	0.705677
-34.004642	-0.193620	0.710682
-34.524069	-0.575999	0.715686
-34.959368	-2.841846	0.720691
-34.703820	0.731634	0.725696
-35.262515	0.733059	0.730701
-36.140113	0.138861	0.735706
-36.405367	0.021635	0.740710
-36.626241	2.961841	0.745715
-36.602594	-3.184596	0.750720
-36.532551	-2.937229	0.755725
-36.588606	-0.801220	0.760730
-36.533682	-1.293519	0.765734
-37.257507	2.231603	0.770739
-37.771218	-6.158712	0.775744
-38.293861	-9.000118	0.780749
-38.624419	-5.387787	0.785754
-38.068605	2.403689	0.790758
-38.890573	5.735497	0.795763
-38.457635	0.629696	0.800768
-39.360606	7.189873	0.805773
-39.713857	-5.617879	0.810778
-39.748076	-2.055019	0.815782
-40.241856	-0.049573	0.820787
-40.262432	1.054231	0.825792
-40.458335	-0.920137	0.830797
-40.180861	-2.781489	0.835802
-40.177821	-6.143299	0.840806
-41.271616	-3.453982	0.845811
-41.522551	-8.957023	0.850816
-41.518484	2.420400	0.855821
-41.776277	-2.598238	0.860826
-42.838918	0.514528	0.865830
-42.768650	2.333814	0.870835
-42.786686	-1.368261	0.875840
-43.370310	2.576064	0.880845
-43.286636	0.059693	0.885850
-43.228406	-7.681396	0.890854
-43.349785	1.729461	0.895859
-43.751293	-13.357580	0.900864
-44.070050	0.507803	0.905869
-44.838695	2.333219	0.910874
-44.590757	-11.982261	0.915878
-44.881271	5.104449	0.920883
-44.848060	-5.308336	0.925888
-45.164249	-1.401199	0.930893
-45.747608	1.194507	0.935898
-46.414255	-2.614057	0.940902
-46.588806	7.483646	0.945907
-46.714539	-3.664918	0.950912
-46.716866	-2.090734	0.955917
-46.571353	2.983729	0.960922
-46.393707	-7.718190	0.965926
-47.518963	1.483201	0.970931
-47.521011	-8.549401	0.975936
-48.007507	-7.641346	0.980941
-48.084969	-11.405405	0.985946
-47.949687	-6.488893	0.990950
-49.066415	7.698684	0.995955
-49.558913	-4.338704	1.000960
-49.606692	-9.303321	1.005965
-49.588686	3.638618	1.010970
-49.758627	-4.746075	1.015974
-49.940172	-0.341659	1.020979
-49.773439	-10.489828	1.025984
-49.933184	0.184393	1.030989
-50.679909	6.540305	1.035994
-50.965774	1.901446	1.040998
-51.226696	6.758076	1.046003
-50.878180	-8.511199	1.051008
-52.080062	-1.384113	1.056013
-52.403776	-7.782831	1.061018
-52.522326	-9.997731	1.066022
-52.944062	-5.584518	1.071027
-52.766783	-13.504370	1.076032
-52.941237	0.610419	1.081037
-52.969534	-5.115579	1.086042
-53.038537	-9.232687	1.091046
-53.598135	-11.924311	1.096051
-54.029083	-10.484171	1.101056
-54.531838	-7.597528	1.106061
-54.500937	-5.886966	1.111066
-54.231437	-8.161002	1.116070
-54.550014	0.029053	1.121075
-54.996070	-8.544537	1.126080
-55.870383	-11.086754	1.131085
-56.077363	-7.752606	1.136090
-55.967205	-13.344059	1.141094
-56.106551	-3.854653	1.146099
-55.989944	-11.229093	1.151104
-57.046444	-4.186863	1.156109
-57.456225	-8.284631	1.161114
-57.558111	-10.821574	1.166118
-57.969994	-5.663680	1.171123
-57.616041	-12.898250	1.176128
-57.625582	-14.131710	1.181133
-57.961544	-14.416600	1.186138
-57.587428	-13.221088	1.191142
-58.679626	-10.542886	1.196147
-59.019421	-8.851640	1.201152
-59.206598	-1.969565	1.206157
-59.301113	-1.295148	1.211162
-59.944656	-8.398458	1.216166
-60.516384	-3.218628	1.221171
-60.420443	-5.804715	1.226176
-60.537407	-9.773772	1.231181
-60.641581	-3.409433	1.236186
-60.636608	-2.991450	1.241190
-60.847167	-0.297251	1.246195
-61.492308	1.738989	1.251200
-61.994978	-2.498105	1.256205
-62.273981	-3.127894	1.261210
-62.300250	-4.895134	1.266214
-62.634989	-7.977224	1.271219
-62.350988	-2.209578	1.276224
-62.307399	-0.875261	1.281229
-63.348082	-3.680989	1.286234
-63.612733	-10.078042	1.291238
-63.893805	-2.456007	1.296243
-63.615101	1.109294	1.301248
-64.006994	-5.787647	1.306253
-64.898578	1.617599	1.311258
-65.178324	-3.631240	1.316262
-65.659663	-1.514188	1.321267
-65.203822	-9.794134	1.326272
-65.623716	-8.763908	1.331277
-65.730607	-8.502236	1.336282
-65.862471	-13.531462	1.341286
-65.638915	-5.327006	1.346291
-66.233581	-4.022155	1.351296
-66.808234	-3.324852	1.356301
-67.161663	-8.424537	1.361306
-67.054458	1.949333	1.366310
-67.128155	-5.590727	1.371315
-67.154088	1.399620	1.376320
-67.833992	-5.515923	1.381325
-68.399346	-8.037478	1.386330
-68.534586	-1.879337	1.391334
-69.041971	3.933934	1.396339
-68.860967	-0.068688	1.401344
-69.755955	4.224589	1.406349
-70.001917	3.391600	1.411354
-70.080646	-6.105960	1.416358
-70.425000	-6.736370	1.421363
-70.374941	-7.220957	1.426368
-70.597454	-0.454192	1.431373
-70.575547	-1.093561	1.436378
-70.602461	-4.117705	1.441382
-70.904134	6.300995	1.446387
-71.312963	-0.147958	1.451392
-71.890267	-6.268862	1.456397
-72.513089	-9.871754	1.461402
-72.328261	-6.576449	1.466406
-72.264321	11.201424	1.471411
-72.183089	-10.639570	1.476416
-72.857525	-12.070552	1.481421
-73.272052	-1.253694	1.486426
-73.226111	-8.597290	1.491430
-73.403878	-8.283228	1.496435
-74.146028	-14.133119	1.501440
-74.958535	-4.744358	1.506445
-74.938423	-6.180655	1.511450
-74.914627	-13.836313	1.516454
-75.056460	-0.237035	1.521459
-75.152321	-3.579504	1.526464
-75.154828	-5.565574	1.531469
-75.487136	-17.403333	1.536474
-75.767723	-11.766354	1.541478
-76.596032	-8.452436	1.546483
-76.390218	-7.890314	1.551488
-76.811515	-9.483003	1.556493
-76.880900	5.201847	1.561498
-77.120065	-8.469967	1.566502
-77.814104	-2.532445	1.571507
-78.084165	-9.323266	1.576512
-78.377756	-13.367062	1.581517
-78.820216	-6.847045	1.586522
-78.602264	-14.136641	1.591526
-78.998224	-8.747347	1.596531
-78.812629	-4.388939	1.601536
-78.815224	-11.992867	1.606541
-79.412190	-13.520742	1.611546
-79.692072	-15.969399	1.616550
-79.987546	-10.446775	1.621555
-80.095147	-11.011809	1.626560
-80.284910	-11.997368	1.631565
-80.847271	-8.448468	1.636570
-81.215734	-20.755215	1.641574
-81.734078	-12.655019	1.646579
-81.814692	-11.300527	1.651584
-81.751759	-12.448311	1.656589
-81.860351	-15.664151	1.661594
-81.738322	-11.792496	1.666598
-82.283696	-18.639144	1.671603
-82.834692	-14.090860	1.676608
-83.020587	-16.141078	1.681613
-83.139940	-14.230400	1.686618
-83.253542	-18.158374	1.691622
-83.809994	-14.923226	1.696627
-84.557543	-15.397859	1.701632
-84.585256	-24.553984	1.706637
-85.126326	-15.548018	1.711642
-84.837947	-18.389158	1.716646
-85.142679	-4.255365	1.721651
-85.403953	-10.285934	1.726656
-85.132339	-15.518341	1.731661
-85.288404	-10.052156	1.736666
-85.494028	-10.635884	1.741670
-86.195588	-9.862504	1.746675
-86.242208	-13.692249	1.751680
-86.658554	-12.208152	1.756685
-87.374082	-3.999715	1.761690
-87.567761	-13.095009	1.766694
-87.992861	-16.230801	1.771699
-88.040594	-11.664242	1.776704
-88.012493	-11.469524	1.781709
-87.972033	-16.904589	1.786714
-87.899057	-18.897634	1.791718
-88.853151	-10.187337	1.796723
-88.804664	-25.548783	1.801728
-89.246026	-17.456998	1.806733
-89.330871	-16.714722	1.811738
-89.616931	-19.999833	1.816742
-90.650629	-11.410736	1.821747
-90.678360	-16.066685	1.826752
-90.997421	-17.900671	1.831757
-91.189336	-15.925485	1.836762
-91.105898	-10.134100	1.841766
-91.260462	-4.378279	1.846771
-91.047095	-20.397911	1.851776
-91.385451	-14.717425	1.856781
-92.319639	-12.820184	1.861786
-92.342903	-14.341056	1.866790
-92.518029	-10.010719	1.871795
-93.149723	-15.067862	1.876800
-93.010565	-22.468329	1.881805
-93.024982	-12.796961	1.886810
-93.027646	-19.655349	1.891814
-94.223570	-16.311721	1.896819
-94.390860	-19.060421	1.901824
-94.490273	-15.406256	1.906829
-94.587313	-9.599186	1.911834
-94.403759	-21.339253	1.916838
-94.853326	-5.585446	1.921843
-95.560238	-14.851674	1.926848
-95.630631	-16.836365	1.931853
-95.954608	-4.500245	1.936858
-96.163430	-12.675827	1.941862
-96.302894	-12.542945	1.946867
-96.379037	-15.716404	1.951872
-96.497671	-14.243530	1.956877
-97.410057	-10.836947	1.961882
-97.699744	-14.355298	1.966886
-98.084179	-6.876973	1.971891
-97.795193	-4.921644	1.976896
-97.411582	-16.011090	1.981901
-98.046804	-4.194895	1.986906
-98.424031	-16.580307	1.991910
-99.033330	-5.386651	1.996915
-99.204953	-7.369330	2.006912
-98.961664	-15.931754	2.016909
-98.412220	-7.976150	2.026906
-97.849217	-14.483882	2.036902
-96.849755	-10.318213	2.046899
-96.550623	-8.493328	2.056896
-96.606458	-5.206003	2.066893
-96.144660	-8.686954	2.076890
-95.331008	-2.194760	2.086886
-94.974903	-9.608536	2.096883
-93.920808	-13.350199	2.106880
-93.760904	-10.063832	2.116877
-93.413078	-18.041525	2.126874
-92.648091	-12.317192	2.136870
-91.992241	-17.143831	2.146867
-91.892498	-15.774947	2.156864
-91.530006	-15.262843	2.166861
-90.735342	-11.631903	2.176858
-90.515547	-14.003833	2.186854
-89.612771	-19.684630	2.196851
-88.901837	-17.756644	2.206848
-88.803854	-16.277216	2.216845
-88.504049	-12.571823	2.226842
-87.369736	-13.374448	2.236838
-87.189513	-17.513746	2.246835
-87.106766	-18.537179	2.256832
-86.515355	-13.975932	2.266829
-86.091254	-20.432005	2.276826
-85.434829	-19.054750	2.286822
-84.835733	-18.771712	2.296819
-83.690626	-20.858256	2.306816
-83.733542	-20.517294	2.316813
-83.661950	-23.187334	2.326810
-82.940987	-19.784057	2.336806
-81.954243	-17.005304	2.346803
-81.788422	-16.588266	2.356800
-81.219268	-15.061605	2.366797
-80.557609	-21.585080	2.376794
-80.141903	-18.178269	2.386790
-80.071511	-17.749970	2.396787
-78.889406	-17.626916	2.406784
-78.356489	-12.678789	2.416781
-78.675633	-14.442796	2.426778
-77.962909	-12.277804	2.436774
-76.965065	-11.240035	2.446771
-77.068841	-19.449586	2.456768
-76.160939	-11.676641	2.466765
-75.434223	-8.623446	2.476762
-75.137961	-10.390389	2.486758
-74.924096	-10.784888	2.496755
-74.167234	-7.657256	2.506752
-73.856198	-11.334335	2.516749
-73.380602	-13.876469	2.526746
-72.352114	-6.446940	2.536742
-71.928760	-10.438802	2.546739
-72.142486	-7.205546	2.556736
-71.109942	-6.230823	2.566733
-70.519653	-4.683554	2.576730
-70.733368	-3.068922	2.586726
-69.550352	-3.268475	2.596723
-69.093475	-3.660741	2.606720
-69.057234	-4.263518	2.616717
-67.919656	-1.497095	2.626714
-67.583592	-4.050303	2.636710
-67.571812	-5.015945	2.646707
-66.445205	-4.805649	2.656704
-66.136644	-3.750733	2.666701
-66.196059	-4.650248	2.676698
-65.018155	-1.853554	2.686694
-64.589273	-5.876563	2.696691
-64.295180	-6.887776	2.706688
-63.714812	-6.906705	2.716685
-62.979917	-6.569887	2.726682
-62.723687	-4.270603	2.736678
-62.350337	-5.080364	2.746675
-61.609238	-11.574912	2.756672
-61.572388	-12.456583	2.766669
-60.443350	-9.791094	2.776666
-59.955197	-15.947764	2.786662
-59.657168	-13.632089	2.796659
-59.407613	-9.530707	2.806656
-58.437160	-11.292138	2.816653
-58.200224	-5.023324	2.826650
-58.231504	-12.725236	2.836646
-56.929641	-9.554295	2.846643
-56.743984	-7.484377	2.856640
-56.229473	-9.733021	2.866637
-55.502266	-1.215866	2.876634
-55.329365	-9.248370	2.886630
-54.687902	-11.253273	2.896627
-53.933169	-13.400229	2.906624
-53.793225	-7.644486	2.916621
-53.407932	-8.605402	2.926618
-52.543311	-12.162745	2.936614
-52.422910	-9.107725	2.946611
-51.672606	-15.725706	2.956608
-50.998282	-8.953961	2.966605
-50.692730	-10.654274	2.976602
-50.242908	-9.239041	2.986598
-49.547535	-11.955684	2.996595
-48.887973	-16.076564	3.006592
-48.692655	-13.593515	3.016589
-48.398529	-9.494969	3.026586
-47.401143	-7.179133	3.036582
-47.146137	-12.268363	3.046579
-46.880317	-6.867781	3.056576
-45.973392	-10.484490	3.066573
-45.952563	-10.123460	3.076570
-44.879491	-8.245363	3.086566
-44.119099	-10.582146	3.096563
-44.071201	-18.279980	3.106560
-44.089295	-13.013170	3.116557
-43.697097	-14.164120	3.126554
-42.716624	-10.815666	3.136550
-41.553274	-14.195851	3.146547
-41.595768	-14.510548	3.156544
-41.117873	-13.360579	3.166541
-41.070703	-8.436718	3.176538
-39.994202	-5.308469	3.186534
-39.783644	-6.704969	3.196531
-39.261316	-12.400997	3.206528
-38.370801	-11.889398	3.216525
-38.040593	-13.480379	3.226522
-38.089131	-11.678525	3.236518
-37.089684	-12.074102	3.246515
-36.495361	-16.138732	3.256512
-36.276748	-11.495383	3.266509
-35.276778	-9.467262	3.276506
-34.898365	-12.737801	3.286502
-34.906389	-4.811572	3.296499
-33.918954	-10.014593	3.306496
-33.416187	-9.403014	3.316493
-33.398964	-12.212834	3.326490
-32.901509	-14.429210	3.336486
-32.039237	-16.188921	3.346483
-31.723393	-9.755939	3.356480
-31.101716	-13.324021	3.366477
-30.658112	-15.526933	3.376474
-30.468020	-7.333580	3.386470
-29.025439	-11.312653	3.396467
-28.827255	-10.257831	3.406464
-28.757665	-13.061307	3.416461
-28.310649	-14.025132	3.426458
-27.447821	-10.832251	3.436454
-27.041436	-12.943642	3.446451
-26.944721	-14.287501	3.456448
-25.762390	-8.826888	3.466445
-25.604497	-8.154637	3.476442
-25.257414	-14.477231	3.486438
-24.195852	-15.760569	3.496435
-23.916778	-11.826883	3.506432
-23.943428	-10.237305	3.516429
-23.317836	-4.974545	3.526426
-22.527429	-12.006982	3.536422
-22.346416	-6.361967	3.546419
-21.445567	-4.415034	3.556416
-21.131010	-6.881296	3.566413
-20.607972	0.191739	3.576410
-19.705319	-10.819896	3.586406
-19.516135	-5.391207	3.596403
-19.070981	-6.697731	3.606400
-18.892811	-7.940085	3.616397
-17.766926	-9.985098	3.626394
-17.629595	-10.143450	3.636390
-17.314894	-10.898445	3.646387
-16.560832	-14.017801	3.656384
-15.732968	-13.756832	3.666381
-15.721201	-13.738693	3.676378
-14.924347	-7.125936	3.686374
-14.097129	-6.833641	3.696371
-14.238918	-8.388145	3.706368
-13.938808	-9.425247	3.716365
-12.835416	-9.019434	3.726362
-12.536456	-7.029529	3.736358
-12.355698	-8.982039	3.746355
-11.529502	-12.883134	3.756352
-11.150440	-8.737201	3.766349
-10.522143	-15.501537	3.776346
-9.759367	-11.937219	3.786342
-9.514842	-10.663241	3.796339
-9.393053	-13.503222	3.806336
-8.638149	-16.244932	3.816333
-8.158834	-15.506963	3.826330
-7.536695	-13.564255	3.836326
-6.561286	-10.225425	3.846323
-6.336984	-14.462914	3.856320
-6.162346	-9.533486	3.866317
-5.872971	-14.443466	3.876314
-4.982222	-10.501217	3.886310
-4.800424	-12.737632	3.896307
-4.026459	-7.207408	3.906304
-3.479995	-8.986341	3.916301
-3.237333	4.725187	3.926298
-2.759785	5.603736	3.936294
-2.474769	14.668546	3.946291
-2.271565	36.005361	3.956288
-1.681204	49.007906	3.966285
-0.914698	80.902009	3.976282
-0.490341	96.139329	3.986278
-0.345497	108.619386	3.996275
0.000000	123.832103	4.001280
0.470416	138.157742	4.006285
0.771309	136.711045	4.011290
1.032210	139.926893	4.016294
0.745194	148.083383	4.021299
1.062643	155.431342	4.026304
1.013336	167.779937	4.031309
1.257227	172.478624	4.036314
1.365518	170.410047	4.041318
0.979689	172.632857	4.046323
1.238201	180.747173	4.051328
1.652556	169.752352	4.056333
1.187615	176.141978	4.061338
1.590987	176.994433	4.066342
1.122808	176.144159	4.071347
1.111825	173.573382	4.076352
1.414270	181.602475	4.081357
1.247533	172.118780	4.086362
1.837523	170.197565	4.091366
1.665681	178.674612	4.096371
1.438767	164.162911	4.101376
1.392236	147.057180	4.106381
1.088921	150.824481	4.111386
1.383519	159.556192	4.116390
1.078881	167.565635	4.121395
1.063871	161.508019	4.126400
1.201266	177.027271	4.131405
1.352710	177.012321	4.136410
1.804419	173.344104	4.141414
1.602591	176.118188	4.146419
1.513470	177.197836	4.151424
1.440897	179.731868	4.156429
1.329972	184.124049	4.161434
1.552545	169.346294	4.166438
1.474109	186.517673	4.171443
1.401641	176.108449	4.176448
1.599631	175.884904	4.181453
1.643516	183.507681	4.186458
1.753167	179.699562	4.191462
1.505467	187.094161	4.196467
1.452410	178.916152	4.201472
1.856411	178.496676	4.206477
1.455512	175.744984	4.211482
1.728801	171.698421	4.216486
1.618293	178.015341	4.221491
2.001676	174.317195	4.226496
1.933428	174.134583	4.231501
1.799365	177.148851	4.236506
1.986854	171.742450	4.241510
1.547702	177.088834	4.246515
1.653847	175.076458	4.251520
1.864017	173.017649	4.256525
1.411735	179.082536	4.261530
1.694016	171.959208	4.266534
1.510177	179.437357	4.271539
1.905750	170.374404	4.276544
1.833572	178.383837	4.281549
1.621698	178.159494	4.286554
1.557740	171.475546	4.291558
1.271902	181.043201	4.296563
1.866432	189.822348	4.301568
2.137238	202.643662	4.306573
1.888916	204.267879	4.311578
1.976980	205.678915	4.316582
1.960481	207.311708	4.321587
2.004367	203.746541	4.326592
2.087879	196.394253	4.331597
1.546758	189.082658	4.336602
1.926554	189.221111	4.341606
1.793310	196.746736	4.346611
1.939245	193.574735	4.351616
2.353061	197.462458	4.356621
1.985086	209.066820	4.361626
2.350247	200.697785	4.366630
2.158561	208.878579	4.371635
2.181051	199.378133	4.376640
2.046907	197.081324	4.381645
1.740011	202.755691	4.386650
2.206071	196.842567	4.391654
2.066814	201.653258	4.396659
2.663739	201.373120	4.401664
1.831966	193.374777	4.406669
1.776094	199.370275	4.411674
2.297913	195.907512	4.416678
1.843701	205.533850	4.421683
2.109579	201.531328	4.426688
2.162193	201.680550	4.431693
2.236086	206.666304	4.436698
2.333364	201.148537	4.441702
2.298684	208.594501	4.446707
2.162649	205.965492	4.451712
2.262365	203.786441	4.456717
2.367289	208.098681	4.461722
2.705059	201.280900	4.466726
2.450557	208.751427	4.471731
2.245461	203.370758	4.476736
2.263623	208.418826	4.481741
2.296433	215.243255	4.486746
2.591242	206.719908	4.491750
2.312930	209.674992	4.496755
2.220970	204.827536	4.501760
2.126723	209.199992	4.506765
2.071467	222.251934	4.511770
2.202997	199.675905	4.516774
2.051153	221.958044	4.521779
1.647554	208.275168	4.526784
1.901741	214.313850	4.531789
2.427589	242.462678	4.536794
2.389537	231.685210	4.541798
2.588079	244.370326	4.546803
2.812375	237.851539	4.551808
2.890915	238.991832	4.556813
2.494361	232.848383	4.561818
2.429031	233.357345	4.566822
2.836524	235.001821	4.571827
2.523833	225.165153	4.576832
2.854834	218.377100	4.581837
2.286139	220.559752	4.586842
2.502974	226.621989	4.591846
2.252676	240.828102	4.596851
2.873519	230.839401	4.601856
2.976126	230.991394	4.606861
2.538120	244.506938	4.611866
2.576906	230.771107	4.616870
2.727381	235.103437	4.621875
2.313095	237.929687	4.626880
2.674967	244.133676	4.631885
2.377074	244.797185	4.636890
2.596796	241.052519	4.641894
2.735787	249.680992	4.646899
2.934631	242.412198	4.651904
2.796526	240.363301	4.656909
2.696179	245.985916	4.661914
2.872482	240.269552	4.666918
2.894636	246.620969	4.671923
2.827835	238.491184	4.676928
2.888262	247.579239	4.681933
2.812538	246.257851	4.686938
3.367226	246.055156	4.691942
2.775774	249.793827	4.696947
2.707851	251.675694	4.701952
3.008958	235.526407	4.706957
2.730802	247.514344	4.711962
2.699718	243.118365	4.716966
2.455030	250.422707	4.721971
2.698132	238.740064	4.726976
3.110321	234.868608	4.731981
2.886480	240.629679	4.736986
2.906732	246.345594	4.741990
2.545431	245.598781	4.746995
2.608369	241.292807	4.752000
3.029955	258.659704	4.757005
3.012767	276.038701	4.762010
3.290706	265.270450	4.767014
2.970426	265.651727	4.772019
3.129252	249.661557	4.777024
3.215052	251.308198	4.782029
2.901420	254.721632	4.787034
3.394576	255.700319	4.792038
3.051923	249.070186	4.797043
2.989636	249.441693	4.802048
3.097198	256.150949	4.807053
3.087573	272.617192	4.812058
3.521687	269.726610	4.817062
2.954746	262.215999	4.822067
3.055596	260.876025	4.827072
3.054313	272.053056	4.832077
2.754244	278.889226	4.837082
3.557138	272.730849	4.842086
3.086554	274.237958	4.847091
2.994220	278.266750	4.852096
3.041399	271.311171	4.857101
2.964496	284.881010	4.862106
3.189584	273.646319	4.867110
3.395537	278.940174	4.872115
3.514574	281.047028	4.877120
3.320352	265.899525	4.882125
3.313611	280.553749	4.887130
3.311304	276.662912	4.892134
3.259325	273.882429	4.897139
3.340051	272.989202	4.902144
3.497004	270.385072	4.907149
3.473627	279.560629	4.912154
3.471816	273.000929	4.917158
3.528791	274.855208	4.922163
3.232213	271.605116	4.927168
3.618635	271.618150	4.932173
3.563452	278.166898	4.937178
3.358505	275.754322	4.942182
3.405054	284.776023	4.947187
3.439354	279.115722	4.952192
3.790797	271.721199	4.957197
2.976135	287.647462	4.962202
3.272376	270.882661	4.967206
3.573872	268.528893	4.972211
3.424582	281.827736	4.977216
3.341679	268.371324	4.982221
3.293830	298.005299	4.987226
3.146799	293.818739	4.992230
3.717172	294.462588	4.997235
3.355895	305.821806	5.002240
3.370912	292.621877	5.007245
3.401962	304.671727	5.012250
3.601378	293.341617	5.017254
3.644806	301.018006	5.022259
3.355658	298.976157	5.027264
3.697193	294.127926	5.032269
3.722050	297.021967	5.037274
3.999187	299.936391	5.042278
3.683691	301.057087	5.047283
3.480857	304.391798	5.052288
3.866569	303.884178	5.057293
3.687666	298.127751	5.062298
3.704611	298.626641	5.067302
3.921171	306.707912	5.072307
3.790010	305.002604	5.077312
3.697875	300.738278	5.082317
3.628604	305.620885	5.087322
3.619750	315.165052	5.092326
3.666402	320.834787	5.097331
4.024953	327.919483	5.102336
3.985200	326.112207	5.107341
3.841379	334.639362	5.112346
4.358562	327.662362	5.117350
4.247485	327.488221	5.122355
4.288984	321.468939	5.127360
4.057411	301.865592	5.132365
3.725049	302.972899	5.137370
4.092353	300.631317	5.142374
3.935606	305.092295	5.147379
4.026498	300.302935	5.152384
3.995136	303.678909	5.157389
3.825151	307.102311	5.162394
4.045234	299.297558	5.167398
3.961668	313.054417	5.172403
4.108490	323.881747	5.177408
4.194631	312.548280	5.182413
4.142167	325.842572	5.187418
4.104271	321.541434	5.192422
4.551078	309.969256	5.197427
3.944842	306.058444	5.202432
4.302493	300.126530	5.207437
4.048949	307.420328	5.212442
4.095502	297.897484	5.217446
4.167483	306.420262	5.222451
3.783973	299.366481	5.227456
4.213296	320.357249	5.232461
4.258065	331.436909	5.237466
4.291055	329.998052	5.242470
4.269539	328.045080	5.247475
4.116649	333.053039	5.252480
4.537869	328.289284	5.257485
4.336556	331.874959	5.262490
4.388171	325.548917	5.267494
4.090843	330.784841	5.272499
4.226340	332.243684	5.277504
4.332562	326.280777	5.282509
4.115390	332.481234	5.287514
4.546119	332.486143	5.292518
4.146920	331.942939	5.297523
4.272014	336.060457	5.302528
4.420468	330.033129	5.307533
4.412134	338.470556	5.312538
4.700307	331.376767	5.317542
4.582940	335.297829	5.322547
4.282140	336.205534	5.327552
4.503205	330.430220	5.332557
4.243019	330.528233	5.337562
4.438042	329.691064	5.342566
4.310125	328.504411	5.347571
4.261336	320.569134	5.352576
4.402273	327.211326	5.357581
4.343199	330.066188	5.362586
4.353923	326.567659	5.367590
4.512469	324.745699	5.372595
4.125960	337.896996	5.377600
4.193253	336.582109	5.382605
4.432639	358.980221	5.387610
4.510581	355.593890	5.392614
4.733070	365.880249	5.397619
4.833051	368.095847	5.402624
4.885049	355.437156	5.407629
4.546660	361.518773	5.412634
5.128152	355.230082	5.417638
4.775962	349.620142	5.422643
4.281978	338.635319	5.427648
4.719415	340.302672	5.432653
4.519710	358.070944	5.437658
4.711136	357.571026	5.442662
4.772094	372.566769	5.447667
4.857315	361.988828	5.452672
4.849004	362.401128	5.457677
4.907330	366.683437	5.462682
4.858191	362.794020	5.467686
4.773213	357.275003	5.472691
4.642596	364.332386	5.477696
5.148914	362.636354	5.482701
4.962362	358.237868	5.487706
4.431900	340.835542	5.492710
4.744536	354.846513	5.497715
4.487339	360.643344	5.502720
4.965928	356.211672	5.507725
4.587389	368.791961	5.512730
5.093303	365.788829	5.517734
4.992953	361.505915	5.522739
4.576152	362.700620	5.527744
4.793733	364.762356	5.532749
4.860916	367.130402	5.537754
4.943007	373.438793	5.542758
4.743982	362.051280	5.547763
4.892054	372.265308	5.552768
5.064221	364.189027	5.557773
4.728885	372.037106	5.562778
4.978130	367.033834	5.567782
5.013103	367.065800	5.572787
4.771737	369.650312	5.577792
5.112609	372.203329	5.582797
5.000697	391.193027	5.587802
5.613364	387.213149	5.592806
5.264837	386.599588	5.597811
5.209452	368.842875	5.602816
5.091759	361.751952	5.607821
5.200424	367.749671	5.612826
5.050224	370.598122	5.617830
4.855608	374.264199	5.622835
5.161924	392.738063	5.627840
5.212066	390.882345	5.632845
5.371165	402.607955	5.637850
5.481184	394.408944	5.642854
5.529838	381.384131	5.647859
5.064628	384.009464	5.652864
5.379678	369.754740	5.657869
5.472556	371.866137	5.662874
5.137782	377.901577	5.667878
5.229499	368.666230	5.672883
5.072943	376.031420	5.677888
5.190093	383.876009	5.682893
5.312108	399.690684	5.687898
5.410254	405.645956	5.692902
5.289465	403.886033	5.697907
5.339963	400.530877	5.702912
5.555539	401.157116	5.707917
4.981414	409.634405	5.712922
5.170646	403.191609	5.717926
5.357520	401.598597	5.722931
5.093955	407.773220	5.727936
4.997166	401.610254	5.732941
5.308001	407.805395	5.737946
5.407996	405.205347	5.742950
5.306195	401.842655	5.747955
5.003450	398.982313	5.752960
5.531736	411.945080	5.757965
5.574672	428.678664	5.762970
5.814883	428.736042	5.767974
5.891883	436.365892	5.772979
5.275758	412.273876	5.777984
5.805506	412.794017	5.782989
5.253119	415.822746	5.787994
5.694878	419.255376	5.792998
6.093613	430.026460	5.798003
5.652946	423.588904	5.803008
5.463760	407.200746	5.808013
5.584988	405.030932	5.813018
5.532310	416.412733	5.818022
5.657612	425.010615	5.823027
5.541463	431.881121	5.828032
5.756279	433.977069	5.833037
5.538707	436.306637	5.838042
5.558687	430.609973	5.843046
5.801774	434.299683	5.848051
5.530858	432.754261	5.853056
5.842062	434.235916	5.858061
5.699410	430.121609	5.863066
5.630734	431.862524	5.868070
5.536870	438.208961	5.873075
5.283575	444.483921	5.878080
5.594947	428.770826	5.883085
5.572876	440.441610	5.888090
5.734986	440.894167	5.893094
5.908844	453.589068	5.898099
5.978257	465.365493	5.903104
6.240874	451.290865	5.908109
5.575536	437.836233	5.913114
5.894285	447.064361	5.918118
6.240042	450.848372	5.923123
5.963288	446.960317	5.928128
5.930376	430.311817	5.933133
5.970109	437.195387	5.938138
5.699524	424.600716	5.943142
5.975423	440.900267	5.948147
5.914156	465.296452	5.953152
6.139970	455.524384	5.958157
5.986452	468.194575	5.963162
5.962311	467.340806	5.968166
6.394764	471.133159	5.973171
5.803773	472.240484	5.978176
6.202792	452.856154	5.983181
6.066417	477.586064	5.988186
5.999585	470.141719	5.993190
6.010668	459.387728	5.998195
5.761261	469.359598	6.003200
5.855295	463.325838	6.008205
5.764950	474.886986	6.013210
6.079710	467.466082	6.018214
5.855587	464.058116	6.023219
6.046141	465.839976	6.028224
6.275865	460.053905	6.033229
5.856622	461.108120	6.038234
5.971790	455.016794	6.043238
6.133949	458.909357	6.048243
5.913178	463.848479	6.053248
6.187732	459.493784	6.058253
5.768486	466.305962	6.063258
6.036998	482.932391	6.068262
6.397402	489.775115	6.073267
6.267198	496.205936	6.078272
6.668211	468.688697	6.083277
6.141799	472.308705	6.088282
6.149856	465.500418	6.093286
6.162325	462.553329	6.098291
5.905764	458.753098	6.103296
6.307666	462.170828	6.108301
6.149625	465.392184	6.113306
6.610450	467.428255	6.118310
6.321377	462.386815	6.123315
5.965985	471.852895	6.128320
6.045402	467.830270	6.133325
6.214687	462.845537	6.138330
6.229620	468.631878	6.143334
6.357141	469.073981	6.148339
5.951549	466.384583	6.153344
6.294881	466.172684	6.158349
6.131544	470.707027	6.163354
5.950341	470.348342	6.168358
6.258321	465.848393	6.173363
6.274831	478.514511	6.178368
5.987156	460.169609	6.183373
6.069825	467.840372	6.188378
6.102681	471.081227	6.193382
6.184707	464.705099	6.198387
6.240034	477.687240	6.203392
6.154845	465.453750	6.208397
6.108618	462.587029	6.213402
6.169415	466.320946	6.218406
6.196657	463.365293	6.223411
5.799295	481.127957	6.228416
6.218413	462.614105	6.233421
6.174561	470.851069	6.238426
5.952155	471.234691	6.243430
6.227102	466.605233	6.248435
6.062235	465.785424	6.253440
6.151408	468.077618	6.258445
6.168665	474.178529	6.263450
6.084355	466.046986	6.268454
6.347429	472.694865	6.273459
5.980948	480.423635	6.278464
6.235761	465.069160	6.283469
6.259663	480.278152	6.288474
6.156738	474.782391	6.293478
6.098044	471.945953	6.298483
5.787383	473.726749	6.303488
6.191292	473.143293	6.308493
5.845485	472.560851	6.313498
5.962420	472.421965	6.318502
6.418752	476.788964	6.323507
6.223826	477.407408	6.328512
6.154843	476.736695	6.333517
6.097074	479.850476	6.338522
6.206885	482.515975	6.343526
6.275337	480.085720	6.348531
5.951741	483.245496	6.353536
6.365571	477.857748	6.358541
6.202720	472.067023	6.363546
6.225759	471.643335	6.368550
6.235173	473.966105	6.373555
5.768023	472.175913	6.378560
6.501639	464.252882	6.383565
6.061851	469.907517	6.388570
6.327749	468.760621	6.393574
6.071800	470.425201	6.398579
6.053421	469.790905	6.403584
6.241084	458.693903	6.408589
6.304461	468.108786	6.413594
6.147161	465.733284	6.418598
6.173774	461.812155	6.423603
6.048076	464.931854	6.428608
6.140655	459.185663	6.433613
6.076828	463.488819	6.438618
6.112865	464.785356	6.443622
6.256456	461.335441	6.448627
6.049024	468.435982	6.453632
6.382856	468.874310	6.458637
6.135878	472.927578	6.463642
6.214682	466.319516	6.468646
6.238171	465.854314	6.473651
6.236970	473.391753	6.478656
6.383096	460.027096	6.483661
6.140425	461.070819	6.488666
6.045119	464.486229	6.493670
6.398657	459.359882	6.498675
6.138317	463.842205	6.503680
5.784077	461.014060	6.508685
5.456517	464.429253	6.513690
5.579185	466.789310	6.518694
6.135870	466.770598	6.523699
5.857952	470.400171	6.528704
6.155338	467.888985	6.533709
6.277326	463.609678	6.538714
6.022931	470.591108	6.543718
6.209441	471.788922	6.548723
6.077651	471.352986	6.553728
6.309742	469.969158	6.558733
5.896323	475.305067	6.563738
5.723306	472.451053	6.568742
6.173989	467.159230	6.573747
6.006219	478.090272	6.578752
6.105506	468.254096	6.583757
6.038289	471.939750	6.588762
6.018906	479.859095	6.593766
6.070190	480.107999	6.598771
6.397202	500.788174	6.603776
6.378777	480.727785	6.608781
6.295988	476.684264	6.613786
5.874443	475.153519	6.618790
6.135574	476.754770	6.623795
6.083471	480.233282	6.628800
6.246689	464.943311	6.633805
6.237696	470.863464	6.638810
6.606495	475.215751	6.643814
6.569163	472.934837	6.648819
6.376857	471.179645	6.653824
6.131561	473.643659	6.658829
6.201374	477.141252	6.663834
6.367492	476.315965	6.668838
6.446993	476.321416	6.673843
5.833398	480.354291	6.678848
6.257366	468.875173	6.683853
6.073150	472.123560	6.688858
6.028493	476.466171	6.693862
6.215810	474.843083	6.698867
6.016397	472.350230	6.703872
6.087918	477.096894	6.708877
6.297281	471.475417	6.713882
6.121072	476.654824	6.718886
6.385085	460.785353	6.723891
6.364311	480.399249	6.728896
6.134180	469.154749	6.733901
6.449107	472.669174	6.738906
6.273700	472.157184	6.743910
6.396798	438.389322	6.748915
6.050531	449.371807	6.753920
6.250481	436.917461	6.758925
5.957073	440.043813	6.763930
6.039569	437.750165	6.768934
6.239813	428.045892	6.773939
6.026816	435.268702	6.778944
5.867902	440.133438	6.783949
6.075135	449.884828	6.788954
6.166679	454.976868	6.793958
6.386485	461.979619	6.798963
5.905815	453.186921	6.803968
6.102689	444.753861	6.808973
6.485449	460.873722	6.813978
6.225054	454.252375	6.818982
6.184122	441.123944	6.823987
6.021108	441.973120	6.828992
6.219752	433.095958	6.833997
6.311063	437.581412	6.839002
6.268709	443.868998	6.844006
6.299076	437.775342	6.849011
6.266081	443.626642	6.854016
6.260930	447.880017	6.859021
6.200296	446.385612	6.864026
6.213743	453.464369	6.869030
6.274109	446.346288	6.874035
6.005623	439.837981	6.879040
6.191976	441.913384	6.884045
6.352424	440.409798	6.889050
6.018805	445.650784	6.894054
6.215733	443.209125	6.899059
6.131825	451.408903	6.904064
6.325787	442.914757	6.909069
6.570121	447.911832	6.914074
6.609890	445.792404	6.919078
6.618509	441.328421	6.924083
6.063893	431.429069	6.929088
6.154532	422.231166	6.934093
5.926620	414.975736	6.939098
5.797866	416.653189	6.944102
6.145054	423.062348	6.949107
5.987765	433.774945	6.954112
6.219809	437.896683	6.959117
6.073769	446.587466	6.964122
6.252420	447.865909	6.969126
6.545593	437.356688	6.974131
6.180101	429.203449	6.979136
6.012835	416.037548	6.984141
6.059112	412.047659	6.989146
5.741206	412.981290	6.994150
6.435971	428.443422	6.999155
6.111396	429.571748	7.004160
6.200814	426.378077	7.009165
6.107922	424.856652	7.014170
5.831648	430.790465	7.019174
6.398547	431.596713	7.024179
6.140614	439.144880	7.029184
6.124712	425.808072	7.034189
6.059385	425.031575	7.039194
6.120804	424.308288	7.044198
6.024398	424.596646	7.049203
5.863012	441.835918	7.054208
6.415670	437.372223	7.059213
6.329328	437.753637	7.064218
6.327864	432.266151	7.069222
6.242365	416.987025	7.074227
6.131571	414.144622	7.079232
6.019663	412.351653	7.084237
6.176497	409.929465	7.089242
5.805563	417.055678	7.094246
6.198330	422.805677	7.099251
5.947553	430.697998	7.104256
6.033674	434.737337	7.109261
6.292453	438.622973	7.114266
6.259048	443.496921	7.119270
6.323898	432.141238	7.124275
5.889134	422.513316	7.129280
6.041995	430.586058	7.134285
6.384165	434.052154	7.139290
6.094619	429.090528	7.144294
6.200554	416.532378	7.149299
6.234063	419.742330	7.154304
6.164375	416.944625	7.159309
6.028921	411.513475	7.164314
6.003494	406.215859	7.169318
6.203435	411.994827	7.174323
6.158830	423.289059	7.179328
5.815747	421.138116	7.184333
6.070606	428.405796	7.189338
6.035379	440.834172	7.194342
6.181738	435.106909	7.199347
6.096444	446.045384	7.204352
6.289458	438.027577	7.209357
6.303244	446.191638	7.214362
6.217759	442.077333	7.219366
6.008251	425.155957	7.224371
5.695467	441.659757	7.229376
6.350725	433.879961	7.234381
6.283347	442.605076	7.239386
6.067445	445.918103	7.244390
6.195764	435.242200	7.249395
5.963949	442.850376	7.254400
6.079834	436.951540	7.259405
6.143812	438.743504	7.264410
6.008217	441.196647	7.269414
6.318253	437.737526	7.274419
5.982311	432.755166	7.279424
6.031320	424.625444	7.284429
6.181487	432.626012	7.289434
5.935494	443.497955	7.294438
6.244848	434.358943	7.299443
5.842303	437.281953	7.304448
6.022826	432.847127	7.309453
6.055219	444.140859	7.314458
6.037484	432.303729	7.319462
6.109966	435.593467	7.324467
6.285762	437.042686	7.329472
6.379824	434.485057	7.334477
6.051846	444.604508	7.339482
6.139173	446.176322	7.344486
5.959963	437.045595	7.349491
6.280999	444.405729	7.354496
6.098942	434.475069	7.359501
6.313867	438.644438	7.364506
5.947354	439.710838	7.369510
6.299253	427.797502	7.374515
6.065527	442.135245	7.379520
6.018831	431.350190	7.384525
6.126995	433.312441	7.389530
5.919216	438.063905	7.394534
5.958027	429.084352	7.399539
5.968371	433.193863	7.404544
6.085756	430.136066	7.409549
6.382607	438.343627	7.414554
5.691350	436.034254	7.419558
5.937333	432.140151	7.424563
5.921547	435.567843	7.429568
6.055322	431.967214	7.434573
6.003100	427.954559	7.439578
5.996610	438.074048	7.444582
6.457652	443.295129	7.449587
5.914085	435.194268	7.454592
5.966857	434.467676	7.459597
6.279003	449.225346	7.464602
6.036735	449.978321	7.469606
6.389284	455.938055	7.474611
5.941049	457.450557	7.479616
6.078162	446.235243	7.484621
6.118359	448.581525	7.489626
6.023441	469.308245	7.494630
6.514763	459.973713	7.499635
6.284209	457.360906	7.504640
6.162884	443.306453	7.509645
5.995649	437.766297	7.514650
5.940122	443.556206	7.519654
6.167990	430.033192	7.524659
5.548631	444.398685	7.529664
5.956984	456.577590	7.534669
6.484541	468.091859	7.539674
6.124260	470.901906	7.544678
6.590744	466.920167	7.549683
6.136562	456.668493	7.554688
6.023567	439.580746	7.559693
6.264342	450.609679	7.564698
6.075578	447.325316	7.569702
6.238154	439.718672	7.574707
5.899165	443.829005	7.579712
6.197934	457.121289	7.584717
6.488150	460.040287	7.589722
6.398644	447.955333	7.594726
6.459061	447.791470	7.599731
6.331263	449.618154	7.604736
6.213918	445.514452	7.609741
6.369209	439.038780	7.614746
5.898977	446.394774	7.619750
6.483896	430.446142	7.624755
6.222877	444.267038	7.629760
6.102675	443.534162	7.634765
6.199933	446.040310	7.639770
6.139309	446.129351	7.644774
6.202068	445.613442	7.649779
6.137676	448.213653	7.654784
5.888274	442.516800	7.659789
5.998351	446.376149	7.664794
6.160897	451.920768	7.669798
6.667870	434.854287	7.674803
5.802449	446.485948	7.679808
5.933970	447.899283	7.684813
5.902046	446.053597	7.689818
5.815630	442.072650	7.694822
5.759555	437.506504	7.699827
5.961969	443.371903	7.704832
6.317259	444.219904	7.709837
6.401187	444.549639	7.714842
5.968358	455.321891	7.719846
6.115288	440.738944	7.724851
6.220033	443.727924	7.729856
6.047023	445.018623	7.734861
6.164255	445.389612	7.739866
5.762598	447.605609	7.744870
5.759550	446.117455	7.749875
6.023405	466.283319	7.754880
6.453606	465.816083	7.759885
6.650715	454.789943	7.764890
6.278532	448.785048	7.769894
6.332460	437.996743	7.774899
6.297935	439.453362	7.779904
6.253339	441.465776	7.784909
6.146235	441.342284	7.789914
6.175331	447.722630	7.794918
6.169614	436.853033	7.799923
6.348273	441.636212	7.804928
6.268719	436.528115	7.809933
6.337872	433.035278	7.814938
6.375990	455.790299	7.819942
6.468307	432.863241	7.824947
6.014339	443.701937	7.829952
6.482402	443.399524	7.834957
6.380428	439.659145	7.839962
6.213059	428.566888	7.844966
6.034618	418.909742	7.849971
5.848990	413.750742	7.854976
5.889027	429.443254	7.859981
6.375812	428.261558	7.864986
6.348955	434.079868	7.869990
5.985163	431.662393	7.874995
6.171707	434.086659	7.880000
6.069892	440.333572	7.885005
6.215591	436.884695	7.890010
5.908637	431.770251	7.895014
6.152480	429.839628	7.900019
6.355918	439.907579	7.905024
6.037387	434.115614	7.910029
6.343200	436.095258	7.915034
6.051248	434.779469	7.920038
6.094126	418.679070	7.925043
5.906928	428.683434	7.930048
5.990076	429.556176	7.935053
6.239486	442.203430	7.940058
5.853595	438.430936	7.945062
6.037777	436.124395	7.950067
6.331243	443.707943	7.955072
6.079479	439.990396	7.960077
6.168090	443.453688	7.965082
6.061314	445.069881	7.970086
6.275447	442.769628	7.975091
6.069090	447.921063	7.980096
5.991726	440.772709	7.985101
6.138073	438.259899	7.990106
6.078047	447.671131	7.995110
6.473673	444.935290	8.000115
6.278699	441.811261	8.005133
6.264688	448.025776	8.010150
6.181733	441.379454	8.015168
5.905200	453.542117	8.020186
6.158016	450.471410	8.025203
6.209870	445.835679	8.030221
6.249620	444.555637	8.035238
6.415971	439.551564	8.040256
6.148356	445.215994	8.045274
6.104081	419.496029	8.050291
6.067651	442.142914	8.055309
6.097024	445.746505	8.060326
6.161747	451.261420	8.065344
6.054215	447.103231	8.070362
5.987630	450.404233	8.075379
6.165288	454.091528	8.080397
6.134099	441.061523	8.085414
6.120216	440.704861	8.090432
5.893295	442.734087	8.095450
5.797603	444.228234	8.100467
6.097231	446.105307	8.105485
5.853360	448.950272	8.110502
6.199694	449.242958	8.115520
5.787396	455.423441	8.120538
6.084903	461.789114	8.125555
6.444671	467.870090	8.130573
6.103514	477.523187	8.135590
6.127863	475.030822	8.140608
6.270513	481.070205	8.145626
6.445251	478.980068	8.150643
6.426683	477.751017	8.155661
6.167166	486.447756	8.160678
6.517313	477.775114	8.165696
6.292433	475.755880	8.170714
6.469227	478.202077	8.175731
6.257284	469.650867	8.180749
5.942136	477.834609	8.185766
6.231415	476.902780	8.190784
6.004755	471.841545	8.195802
6.546914	481.801876	8.200819
6.408853	478.628780	8.205837
6.383538	480.609862	8.210854
6.607404	474.538654	8.215872
6.358717	484.678768	8.220890
6.508175	478.491149	8.225907
6.386532	474.671485	8.230925
6.179314	481.597880	8.235942
6.379450	473.862220	8.240960
6.372047	484.728266	8.245978
6.153225	475.443403	8.250995
6.442454	480.005666	8.256013
6.020128	485.440436	8.261030
6.474380	480.667392	8.266048
6.243722	485.806661	8.271066
6.321594	483.832754	8.276083
6.279769	480.223673	8.281101
6.091198	478.343296	8.286118
6.359646	480.600116	8.291136
6.070860	479.765197	8.296154
6.376149	486.774819	8.301171
6.420625	484.391710	8.306189
6.360468	488.155007	8.311206
6.274098	475.843705	8.316224
6.148132	487.500393	8.321242
6.123150	501.091407	8.326259
6.596064	505.344145	8.331277
6.429779	506.039417	8.336294
6.486500	507.739417	8.341312
6.569615	513.760918	8.346330
6.841221	514.740932	8.351347
7.005363	499.057064	8.356365
6.457315	486.796226	8.361382
6.619897	473.156391	8.366400
6.599159	483.504997	8.371418
6.851802	484.205691	8.376435
6.764444	478.810581	8.381453
6.536723	483.007108	8.386470
6.716226	475.610666	8.391488
6.345638	476.296860	8.396506
6.520537	481.614027	8.401523
6.638062	475.350207	8.406541
6.327545	481.936649	8.411558
6.610256	476.291883	8.416576
6.646107	482.195618	8.421594
6.173933	486.961133	8.426611
6.125496	481.573552	8.431629
6.297740	492.506696	8.436646
6.431343	504.922519	8.441664
6.577909	511.405328	8.446682
6.591081	504.805457	8.451699
6.742222	507.545454	8.456717
6.597575	523.277018	8.461734
6.498647	513.733318	8.466752
6.716605	512.789874	8.471770
6.715941	516.314406	8.476787
6.675702	517.314766	8.481805
6.608553	510.949241	8.486822
6.583310	508.676485	8.491840
6.332029	515.733412	8.496858
6.470938	518.515590	8.501875
6.641127	510.884274	8.506893
6.587436	515.369684	8.511910
6.586456	512.678962	8.516928
6.567863	515.633078	8.521946
6.594817	517.482093	8.526963
6.974844	513.272473	8.531981
6.696917	518.299707	8.536998
6.777414	512.030588	8.542016
6.870119	518.825054	8.547034
6.549346	525.009304	8.552051
6.801964	514.589925	8.557069
6.561322	520.510133	8.562087
6.611255	515.916035	8.567104
6.817728	504.000672	8.572122
6.498641	513.050770	8.577139
6.587892	509.137516	8.582157
6.457752	514.048155	8.587175
6.623785	515.264731	8.592192
6.690485	513.322000	8.597210
6.706031	512.370740	8.602227
7.079539	510.067774	8.607245
6.908403	522.258112	8.612263
7.212564	519.184204	8.617280
6.936574	518.088323	8.622298
6.849638	510.777126	8.627315
6.900550	510.758526	8.632333
6.987231	516.479459	8.637351
7.248826	514.455243	8.642368
6.883411	524.836352	8.647386
6.873282	520.065991	8.652403
7.357642	515.586553	8.657421
7.074617	504.108328	8.662439
6.867824	491.578980	8.667456
6.751113	491.763716	8.672474
6.429462	491.628480	8.677491
7.008219	493.959495	8.682509
6.971692	504.639840	8.687527
6.866802	501.577970	8.692544
6.837931	483.442402	8.697562
6.669874	491.924013	8.702579
6.903173	491.008737	8.707597
6.903645	512.578826	8.712615
6.758684	509.020673	8.717632
6.997072	508.684039	8.722650
6.771204	508.160723	8.727667
6.839707	502.846676	8.732685
6.890291	504.918531	8.737703
6.952051	500.259097	8.742720
7.160505	504.469613	8.747738
6.988052	516.105283	8.752755
7.150722	497.869086	8.757773
6.852777	504.534945	8.762791
6.885099	503.670075	8.767808
6.809793	502.968687	8.772826
6.514102	509.087363	8.777843
6.725905	508.542548	8.782861
6.883929	515.517915	8.787879
6.911651	510.465915	8.792896
6.937138	505.930392	8.797914
6.904825	514.687153	8.802931
6.849858	506.122918	8.807949
6.690547	517.612329	8.812967
6.810335	505.052508	8.817984
7.003979	509.067461	8.823002
7.042940	510.896377	8.828019
6.856389	506.591623	8.833037
6.700963	516.976728	8.838055
7.141094	524.355349	8.843072
7.180238	527.819948	8.848090
6.971781	526.100918	8.853107
7.302862	523.684316	8.858125
7.091643	513.716133	8.863143
6.695758	514.152795	8.868160
6.977466	524.694632	8.873178
7.418426	535.281950	8.878195
7.210350	519.914014	8.883213
6.889548	524.228322	8.888231
7.309917	532.220806	8.893248
7.308607	523.653975	8.898266
7.117344	520.749111	8.903283
6.980347	508.631193	8.908301
6.983602	513.233148	8.913319
6.987989	518.987197	8.918336
7.345452	533.345555	8.923354
7.210929	523.535715	8.928371
6.927319	521.232914	8.933389
6.977095	530.584905	8.938407
7.134908	541.706484	8.943424
7.192995	540.061612	8.948442
7.088497	554.896661	8.953459
7.254298	544.989832	8.958477
7.387539	549.026215	8.963495
7.238330	547.440865	8.968512
7.797873	540.950681	8.973530
7.263054	521.394826	8.978547
7.241010	515.231460	8.983565
6.824753	516.566905	8.988583
6.722531	522.854321	8.993600
7.042031	533.838497	8.998618
7.068504	544.386595	9.003635
7.518704	537.468094	9.008653
7.368066	552.074381	9.013671
7.459807	542.795524	9.018688
7.500714	545.502211	9.023706
7.385169	535.630169	9.028723
7.521417	523.636269	9.033741
7.397294	517.834074	9.038759
7.318229	519.320357	9.043776
7.218630	511.111912	9.048794
6.968227	514.605168	9.053811
6.853234	522.389475	9.058829
7.137531	534.107579	9.063847
7.102537	549.797588	9.068864
7.338214	547.830805	9.073882
7.094859	547.020837	9.078899
7.339532	552.465440	9.083917
7.417248	557.423949	9.088935
7.191229	551.707508	9.093952
7.206608	552.284712	9.098970
7.382847	547.284676	9.103987
7.203616	551.973157	9.109005
7.425508	550.490120	9.114023
7.266137	548.997983	9.119040
7.067425	541.439749	9.124058
7.011355	546.980410	9.129075
7.568054	548.623402	9.134093
7.293179	547.750548	9.139111
6.982365	554.785070	9.144128
7.547831	555.259959	9.149146
7.530135	571.520511	9.154163
7.422204	559.994746	9.159181
7.459438	562.208574	9.164199
7.404958	553.543452	9.169216
7.294741	550.265147	9.174234
7.358885	562.714367	9.179251
7.588997	568.861340	9.184269
7.797871	565.105021	9.189287
7.312850	567.652170	9.194304
7.383929	558.436958	9.199322
7.309261	575.578149	9.204339
7.501798	569.793766	9.209357
7.294091	579.372075	9.214375
7.637079	581.230174	9.219392
7.850954	579.460686	9.224410
7.345886	586.558491	9.229427
7.948747	580.110721	9.234445
7.702563	567.327223	9.239463
7.313980	562.757112	9.244480
7.479559	550.635113	9.249498
7.344497	565.233715	9.254515
7.671843	570.706953	9.259533
8.061586	576.009635	9.264551
7.870797	562.821915	9.269568
7.782312	554.032709	9.274586
7.348730	552.605467	9.279603
7.450607	542.953107	9.284621
7.677403	553.168451	9.289639
7.627391	546.659532	9.294656
7.747392	547.166658	9.299674
7.349475	550.043056	9.304691
7.635217	553.836287	9.309709
7.653694	548.445081	9.314727
7.930566	554.518561	9.319744
7.509401	543.522994	9.324762
7.788550	544.234655	9.329779
7.645085	547.015572	9.334797
7.562492	543.965157	9.339815
7.615578	560.736382	9.344832
7.755645	546.143583	9.349850
7.738697	543.736190	9.354867
7.631835	541.430295	9.359885
7.487887	542.392914	9.364903
7.609117	545.501821	9.369920
7.730322	543.228035	9.374938
7.401740	545.619755	9.379955
7.749934	563.821537	9.384973
7.822870	572.514841	9.389991
7.722852	576.417232	9.395008
7.992961	569.784626	9.400026
7.653238	563.234116	9.405043
7.520538	554.806932	9.410061
7.573425	562.953391	9.415079
7.638211	567.417031	9.420096
7.451263	575.508142	9.425114
7.712051	578.216018	9.430131
7.546900	581.337124	9.435149
7.892052	577.687163	9.440167
7.359092	578.904546	9.445184
7.673433	578.579347	9.450202
7.879776	584.715696	9.455219
7.723055	587.497044	9.460237
8.019168	567.925171	9.465255
7.870052	577.357171	9.470272
7.468553	572.589209	9.475290
7.555519	575.009355	9.480307
7.477756	578.666345	9.485325
7.744399	586.211906	9.490343
7.564188	605.775567	9.495360
7.688068	608.056543	9.500378
7.765900	603.274543	9.505395
7.895268	610.630461	9.510413
7.943479	610.558768	9.515431
7.574292	618.682049	9.520448
8.247245	614.429995	9.525466
7.847525	612.385763	9.530483
7.704575	613.111819	9.535501
7.886190	614.631709	9.540519
7.760206	618.663796	9.545536
7.891492	611.954759	9.550554
8.133022	613.236789	9.555571
7.487307	623.659263	9.560589
7.930862	611.826398	9.565607
7.416597	615.961759	9.570624
7.819365	605.672168	9.575642
7.873633	617.465631	9.580659
7.931495	620.306325	9.585677
7.955756	625.597703	9.590695
7.921713	639.846990	9.595712
8.222651	637.513113	9.600730
8.297850	628.432405	9.605747
7.651766	618.371612	9.610765
8.070369	633.505321	9.615783
7.942087	638.468837	9.620800
8.258180	647.285291	9.625818
8.222874	635.710832	9.630835
7.964108	624.456045	9.635853
8.310381	617.833835	9.640871
7.953319	611.728076	9.645888
8.017486	619.680781	9.650906
8.200448	607.684001	9.655923
8.212365	619.564001	9.660941
8.481212	602.092528	9.665959
7.758576	617.796487	9.670976
7.925405	617.490204	9.675994
8.042988	621.659899	9.681011
8.197854	634.698445	9.686029
8.076409	630.258670	9.691047
8.261573	647.442734	9.696064
8.243414	634.435604	9.701082
8.421880	621.599847	9.706099
8.276029	614.606409	9.711117
8.424641	609.701472	9.716135
8.316683	610.968548	9.721152
8.450803	616.545254	9.726170
8.213439	614.627274	9.731187
8.358293	618.923939	9.736205
8.047311	617.283488	9.741223
8.246875	618.387834	9.746240
8.156210	623.422277	9.751258
8.422033	612.763653	9.756275
8.095685	617.826494	9.761293
8.326044	611.167975	9.766311
7.806459	607.422445	9.771328
8.057685	617.285777	9.776346
8.302239	620.999433	9.781363
8.300715	611.799165	9.786381
8.413518	612.054549	9.791399
8.200917	614.061742	9.796416
8.260063	613.682352	9.801434
8.441697	613.897993	9.806451
8.209938	619.428604	9.811469
8.357271	611.041427	9.816487
8.709376	608.655382	9.821504
8.607772	614.641572	9.826522
8.639615	607.808462	9.831539
8.501644	611.829148	9.836557
8.351944	610.667468	9.841575
8.328438	610.224605	9.846592
8.160304	608.618763	9.851610
8.159552	613.552885	9.856627
8.217185	613.233585	9.861645
8.089506	608.675171	9.866663
8.290849	619.517962	9.871680
8.176149	619.522850	9.876698
8.113332	609.144228	9.881715
8.088621	631.250114	9.886733
8.177222	635.976151	9.891751
8.582311	647.039535	9.896768
8.394222	653.670731	9.901786
8.475553	646.775081	9.906803
8.485496	647.300240	9.911821
8.569883	649.165741	9.916839
8.439647	648.798816	9.921856
8.184102	643.184863	9.926874
8.295941	643.944313	9.931891
8.365465	651.430821	9.936909
8.353847	639.991403	9.941927
8.360167	654.295432	9.946944
8.172874	644.735382	9.951962
8.058385	646.335017	9.956979
8.395305	647.507165	9.961997
8.278484	645.306637	9.967015
8.503521	673.172435	9.972032
8.563261	675.717571	9.977050
8.715102	672.935967	9.982067
8.592883	678.594513	9.987085
8.528754	663.826574	9.992103
8.380271	671.340534	9.997120
8.451176	676.416737	10.002138
8.781444	676.510921	10.007155
9.033976	677.384860	10.012173
8.882177	665.374578	10.017191
8.888075	652.899636	10.022208
8.653534	654.353416	10.027226
8.695369	638.757373	10.032243
8.364590	649.577683	10.037261
8.411451	646.131227	10.042279
8.721938	643.359575	10.047296
8.424174	644.007733	10.052314
8.718359	642.024164	10.057331
8.492637	658.808990	10.062349
8.691919	668.949838	10.067367
8.656929	679.851492	10.072384
8.696376	678.074660	10.077402
8.779614	671.797150	10.082419
8.683083	683.169206	10.087437
8.919628	681.166045	10.092455
8.911014	659.435796	10.097472
8.584612	650.870765	10.102490
8.555847	641.181321	10.107507
8.394526	660.176603	10.112525
8.721220	670.148724	10.117543
8.974740	677.495333	10.122560
8.772998	677.394171	10.127578
9.232054	676.511179	10.132595
8.676785	668.166705	10.137613
8.771147	673.090213	10.142631
8.824963	677.279931	10.147648
8.495072	684.521989	10.152666
8.870154	676.332480	10.157683
8.895503	683.483820	10.162701
8.917219	680.198599	10.167719
8.862813	677.477919	10.172736
8.789530	679.767148	10.177754
8.788573	677.040767	10.182771
8.840464	682.553166	10.187789
8.731380	685.207358	10.192807
8.873966	681.464351	10.197824
8.613256	685.268388	10.202842
8.725967	680.243398	10.207859
8.675402	684.136249	10.212877
8.670915	674.963598	10.217895
8.692228	684.402871	10.222912
9.113666	678.987012	10.227930
9.168553	672.307135	10.232947
8.904678	677.399411	10.237965
9.084794	674.497383	10.242983
9.390979	678.563818	10.248000
8.886287	679.665510	10.253018
8.885243	677.390297	10.258035
8.661840	685.878817	10.263053
8.634301	679.751530	10.268071
8.941571	675.797012	10.273088
8.680501	681.740741	10.278106
8.708523	674.320475	10.283123
8.978547	682.483595	10.288141
8.777810	694.569331	10.293159
9.245162	705.666144	10.298176
9.219623	717.867758	10.303194
9.253745	707.900551	10.308211
8.994349	693.135001	10.313229
9.073894	684.483436	10.318247
9.169138	687.751390	10.323264
8.806079	701.251330	10.328282
9.295694	706.351900	10.333299
9.283882	701.900641	10.338317
9.127962	703.467382	10.343335
9.517026	682.384982	10.348352
9.100628	688.071776	10.353370
8.916341	680.333144	10.358387
9.211454	682.046437	10.363405
9.108543	679.491654	10.368423
9.093566	682.705030	10.373440
8.909180	683.086397	10.378458
9.340078	687.566800	10.383475
9.520959	710.286745	10.388493
9.196972	693.596965	10.393511
9.162592	684.764672	10.398528
9.011211	687.104234	10.403546
9.455073	685.332867	10.408563
9.449091	679.380740	10.413581
9.245204	676.790320	10.418599
9.264165	672.898113	10.423616
8.884670	682.926168	10.428634
9.211316	675.756823	10.433651
9.109232	681.195514	10.438669
9.161112	695.012931	10.443687
9.310220	697.010232	10.448704
9.505617	705.068406	10.453722
9.656412	706.422947	10.458739
9.258125	693.275186	10.463757
9.224808	686.337484	10.468775
9.476895	671.308523	10.473792
8.968130	682.724831	10.478810
9.550197	688.662395	10.483827
9.171910	676.456162	10.488845
9.291411	687.923934	10.493863
9.600508	693.954733	10.498880
8.953616	692.761610	10.503898
9.492316	699.688585	10.508915
9.402106	698.612316	10.513933
9.269894	699.325968	10.518951
9.545845	700.743635	10.523968
9.180804	707.999005	10.528986
9.560391	710.522280	10.534003
9.425155	707.846868	10.539021
9.459725	707.402652	10.544039
9.550644	698.415357	10.549056
9.246801	708.909612	10.554074
9.037551	703.286396	10.559091
9.126152	705.461818	10.564109
8.987596	710.369188	10.569127
9.238044	703.560855	10.574144
9.191530	711.836249	10.579162
9.113647	701.966722	10.584179
9.323567	727.552186	10.589197
9.403681	733.023317	10.594215
9.673670	739.328311	10.599232
9.508242	744.461784	10.604250
9.483432	733.242579	10.609267
9.768429	741.994950	10.614285
9.623704	744.132643	10.619303
9.762002	736.048846	10.624320
9.228106	738.994644	10.629338
9.627600	743.873549	10.634355
9.817914	738.274698	10.639373
9.428651	749.392540	10.644391
9.440715	741.602858	10.649408
9.421805	738.978646	10.654426
9.423906	732.575973	10.659443
9.532230	737.386565	10.664461
9.277095	741.350707	10.669479
9.695931	733.821207	10.674496
9.331256	741.160385	10.679514
9.485681	733.506571	10.684531
9.622570	739.990685	10.689549
9.324609	745.078786	10.694567
9.919593	751.532317	10.699584
9.632248	755.519118	10.704602
9.648760	762.032230	10.709619
9.858085	767.160734	10.714637
9.360811	762.122171	10.719655
10.068579	763.473059	10.724672
9.830937	773.449730	10.729690
9.839120	764.525702	10.734707
9.719296	752.208894	10.739725
9.429133	755.364712	10.744743
10.173978	751.868391	10.749760
10.060321	752.523464	10.754778
9.935837	740.570014	10.759795
9.716892	735.289711	10.764813
9.855441	746.910269	10.769831
9.923643	733.446259	10.774848
9.883626	747.500583	10.779866
9.796138	743.575201	10.784883
9.734739	734.870969	10.789901
9.687669	741.119814	10.794919
9.820577	745.984603	10.799936
9.691910	750.571862	10.804954
9.690465	763.569083	10.809971
10.141085	759.851421	10.814989
9.926132	776.576326	10.820007
9.799956	776.114636	10.825024
9.794970	768.334457	10.830042
9.423482	782.489370	10.835059
9.936864	779.637640	10.840077
9.871057	773.787111	10.845095
10.113445	762.613396	10.850112
10.080201	779.158221	10.855130
9.846917	767.546767	10.860147
10.104696	772.268057	10.865165
9.822359	775.043076	10.870183
10.048971	778.847139	10.875200
9.967907	782.085652	10.880218
9.890517	777.525554	10.885235
10.007747	768.842899	10.890253
9.801317	781.262697	10.895271
10.083713	775.466310	10.900288
10.023716	778.985176	10.905306
9.894063	777.415461	10.910323
10.134891	770.519326	10.915341
9.938663	772.582880	10.920359
9.676149	771.783551	10.925376
9.801074	781.092738	10.930394
9.952232	796.881887	10.935411
10.503246	805.559140	10.940429
10.561550	802.949294	10.945447
10.080175	783.381303	10.950464
10.040706	778.433055	10.955482
9.895920	782.257287	10.960499
10.000472	788.001540	10.965517
10.188676	806.002555	10.970535
10.230407	802.041981	10.975552
10.605808	801.346450	10.980570
9.741342	794.096757	10.985587
10.256927	798.111224	10.990605
10.175012	814.114569	10.995623
10.361139	806.570424	11.000640
10.342291	806.722817	11.005658
10.534626	806.670167	11.010675
10.390746	788.079297	11.015693
10.115423	788.833187	11.020711
10.396773	788.129610	11.025728
10.158715	780.563603	11.030746
9.895536	807.233789	11.035763
10.146008	804.535429	11.040781
10.112375	814.654711	11.045799
10.705596	812.625537	11.050816
10.781810	808.383674	11.055834
10.148183	808.766215	11.060851
10.448893	810.291598	11.065869
10.699969	821.025512	11.070887
10.562562	792.945473	11.075904
10.484134	780.073785	11.080922
10.321281	775.565633	11.085939
10.630061	773.789855	11.090957
10.491393	782.052202	11.095975
10.357422	774.910275	11.100992
10.414827	777.806189	11.106010
10.005419	781.506535	11.111027
10.562154	766.530963	11.116045
10.480565	776.302669	11.121063
10.202497	769.740089	11.126080
10.382732	787.064093	11.131098
10.486807	805.327057	11.136115
10.557454	803.782434	11.141133
10.551787	807.873381	11.146151
10.620160	801.803388	11.151168
10.658533	801.336100	11.156186
10.338277	797.162653	11.161203
10.546928	795.024734	11.166221
10.462843	807.303040	11.171239
10.341097	805.867832	11.176256
10.590315	810.489375	11.181274
10.457492	813.085319	11.186291
10.589332	805.539929	11.191309
10.356215	809.616184	11.196327
10.508870	810.066536	11.201344
10.652497	804.429332	11.206362
10.278190	806.910942	11.211379
10.486162	801.975250	11.216397
10.418538	803.339987	11.221415
10.292048	810.686995	11.226432
10.350668	807.597593	11.231450
10.052932	823.183168	11.236467
10.289793	825.486804	11.241485
10.412721	832.719687	11.246503
10.476829	834.067729	11.251520
10.689064	828.093974	11.256538
10.663866	837.548128	11.261555
10.877413	822.891527	11.266573
10.678928	840.168469	11.271591
10.184353	840.600814	11.276608
10.714485	835.966862	11.281626
10.552234	843.934737	11.286643
10.920527	833.925101	11.291661
10.825108	847.435567	11.296679
10.885919	834.968707	11.301696
10.884101	829.402428	11.306714
10.893972	839.283824	11.311731
10.769028	835.678386	11.316749
10.527692	836.266422	11.321767
10.723499	841.792444	11.326784
10.812490	838.596437	11.331802
10.867156	861.902831	11.336819
10.980521	860.990466	11.341837
10.787581	863.808174	11.346855
11.416205	855.963967	11.351872
10.981863	843.878690	11.356890
10.894655	847.817018	11.361907
11.076550	842.223067	11.366925
10.940060	845.909726	11.371943
11.023596	845.238904	11.376960
11.410685	837.677213	11.381978
10.952167	839.904677	11.386995
11.007385	834.637202	11.392013
10.824178	837.374951	11.397031
10.959242	837.379421	11.402048
10.799596	837.256720	11.407066
10.674303	836.730318	11.412083
10.891039	839.877404	11.417101
10.877673	841.925644	11.422119
11.114199	860.041154	11.427136
11.358631	859.802327	11.432154
11.228444	853.618745	11.437171
10.930815	839.391251	11.442189
10.990536	829.851988	11.447207
10.962700	837.883423	11.452224
11.394121	843.810957	11.457242
11.236694	837.135855	11.462259
11.300493	830.983540	11.467277
11.351183	835.127364	11.472295
11.002333	835.062372	11.477312
11.328554	824.078657	11.482330
11.267026	835.336371	11.487347
11.190304	831.995376	11.492365
10.981030	834.056767	11.497383
10.953484	843.880586	11.502400
10.906689	825.482246	11.507418
11.030018	853.788419	11.512435
11.496739	854.691856	11.517453
11.668772	839.491747	11.522471
11.171076	834.764632	11.527488
11.175751	839.127483	11.532506
10.777958	842.442081	11.537523
10.899559	854.237564	11.542541
11.241766	860.478683	11.547559
11.088151	866.839313	11.552576
11.222617	870.300408	11.557594
11.133704	870.764783	11.562611
11.418617	868.809491	11.567629
11.481300	865.622166	11.572647
10.761960	870.893469	11.577664
11.518974	870.965407	11.582682
11.206286	869.668894	11.587699
11.108374	870.378449	11.592717
11.298556	868.806544	11.597735
11.240227	873.304636	11.602752
11.732920	878.215392	11.607770
11.154197	877.019231	11.612787
11.355729	868.771751	11.617805
11.609384	865.081170	11.622823
11.261713	874.067908	11.627840
11.607931	868.175094	11.632858
11.542059	871.668184	11.637875
11.296086	873.540786	11.642893
11.478285	869.399066	11.647911
11.354925	877.103050	11.652928
11.479324	868.080980	11.657946
11.556360	882.362093	11.662963
11.635321	886.072922	11.667981
11.696842	875.720379	11.672999
11.384815	878.842443	11.678016
11.560157	880.308283	11.683034
11.817133	877.961967	11.688051
11.625568	867.217897	11.693069
11.623171	862.209548	11.698087
11.810311	865.567042	11.703104
11.575793	867.936540	11.708122
11.649092	867.156395	11.713139
11.766296	872.224601	11.718157
11.786016	870.689192	11.723175
11.261767	869.530072	11.728192
11.699054	863.701309	11.733210
11.466686	862.814310	11.738227
11.624341	883.108945	11.743245
12.381070	882.343963	11.748263
11.745941	887.541880	11.753280
11.938740	869.254197	11.758298
12.045806	869.597145	11.763315
11.798848	875.193746	11.768333
12.045450	873.899492	11.773351
11.640621	872.249358	11.778368
11.693202	869.702650	11.783386
11.874989	870.012359	11.788403
11.796024	871.344730	11.793421
11.792683	869.998171	11.798439
11.799786	864.624486	11.803456
11.977918	870.790423	11.808474
11.738609	869.898668	11.813491
11.374332	875.352894	11.818509
11.820455	861.876186	11.823527
11.435829	872.655963	11.828544
11.627265	874.285665	11.833562
11.720514	885.362281	11.838579
11.549930	890.014394	11.843597
12.220869	884.374085	11.848615
11.861704	898.659340	11.853632
11.936348	896.797525	11.858650
11.729276	895.520526	11.863667
12.001419	900.800475	11.868685
12.432199	898.457655	11.873703
12.053775	898.563694	11.878720
12.010307	897.123388	11.883738
11.972470	892.888973	11.888755
11.800654	902.276112	11.893773
11.950197	896.922134	11.898791
11.992362	906.969871	11.903808
12.139431	905.684617	11.908826
12.007620	906.106493	11.913843
12.250761	902.086163	11.918861
12.127866	902.708128	11.923879
12.112761	901.651295	11.928896
12.134252	902.534376	11.933914
12.324628	899.712887	11.938931
12.154122	899.783707	11.943949
12.074232	898.689968	11.948967
12.226092	897.796816	11.953984
12.162398	891.612050	11.959002
12.246691	901.274479	11.964019
11.733389	905.525104	11.969037
12.113199	899.110992	11.974055
12.161765	905.516499	11.979072
12.009569	897.929916	11.984090
11.898499	901.357666	11.989107
11.553947	904.024907	11.994125
12.195634	907.635861	11.999143
12.202408	909.137099	12.004160
12.179670	900.198035	12.009178
12.043671	902.820109	12.014195
11.771839	924.742936	12.019213
12.212284	933.262202	12.024231
12.261808	932.477330	12.029248
12.347692	937.179501	12.034266
12.276517	936.590987	12.039283
12.060821	943.279237	12.044301
12.096661	943.143453	12.049319
12.199982	952.986612	12.054336
12.346466	946.850086	12.059354
12.429799	947.444594	12.064371
12.215442	952.104761	12.069389
12.405047	937.063058	12.074407
12.476392	947.213464	12.079424
12.142558	948.303414	12.084442
12.474610	935.822263	12.089459
12.507069	943.360325	12.094477
12.449597	935.081689	12.099495
12.542278	938.729632	12.104512
12.308323	934.824914	12.109530
12.548930	938.789684	12.114547
12.159304	942.796226	12.119565
12.484036	940.130819	12.124583
12.809510	955.151925	12.129600
12.862265	944.372460	12.134618
12.663975	941.265342	12.139635
12.089758	938.339372	12.144653
12.570337	938.653144	12.149671
12.803208	942.225906	12.154688
12.389832	940.131530	12.159706
12.653372	946.014467	12.164723
12.561999	947.335907	12.169741
12.706449	952.569306	12.174759
12.805026	956.210765	12.179776
12.543923	954.225023	12.184794
12.639450	945.271073	12.189811
12.401438	954.208596	12.194829
12.852370	965.649640	12.199847
12.732506	962.315760	12.204864
12.892805	968.404771	12.209882
13.061604	964.164463	12.214899
12.826109	957.490820	12.219917
12.644442	941.313402	12.224935
12.821911	943.702872	12.229952
12.564835	941.353882	12.234970
12.992727	950.083888	12.239987
12.594559	957.786178	12.245005
12.558194	960.885836	12.250023
12.377924	965.865939	12.255040
12.316550	967.324927	12.260058
12.824847	969.641112	12.265075
12.651164	973.246956	12.270093
12.981461	972.671481	12.275111
13.012803	968.511806	12.280128
12.631032	972.730826	12.285146
13.012176	972.586675	12.290163
12.601667	977.626563	12.295181
12.865219	959.579409	12.300199
12.729466	966.929993	12.305216
12.909130	972.689040	12.310234
13.126427	964.150723	12.315251
13.038521	974.565698	12.320269
13.098785	968.031254	12.325287
12.956933	963.579015	12.330304
12.717299	965.409634	12.335322
13.012553	971.381814	12.340339
12.955441	994.757703	12.345357
13.219842	993.598281	12.350375
13.251976	992.064741	12.355392
13.012122	989.762496	12.360410
12.961739	982.220033	12.365427
12.917394	989.759419	12.370445
13.140227	996.744348	12.375463
13.106968	996.732600	12.380480
13.140356	1002.862325	12.385498
13.345058	999.699483	12.390515
13.434791	1002.075145	12.395533
13.355152	994.543426	12.400551
13.166884	969.556012	12.405568
13.105852	968.265452	12.410586
13.589494	972.232502	12.415603
13.290728	972.154884	12.420621
12.986932	965.031544	12.425639
13.152565	963.357794	12.430656
13.034306	972.895549	12.435674
13.285481	982.528817	12.440691
13.343193	991.019374	12.445709
13.246510	996.240753	12.450727
13.189393	993.480704	12.455744
13.212076	1002.758926	12.460762
13.394144	993.081196	12.465779
13.421081	1000.376902	12.470797
13.284886	999.788523	12.475815
13.759367	998.507701	12.480832
13.255674	992.656772	12.485850
13.661253	987.374531	12.490867
13.309317	995.803012	12.495885
13.492583	1000.250109	12.500903
13.283633	997.671890	12.505920
13.180203	996.218277	12.510938
13.389728	995.949797	12.515955
13.364490	1003.869869	12.520973
13.151130	996.814999	12.525991
13.135155	990.062471	12.531008
13.303759	1007.159916	12.536026
13.429341	988.696617	12.541043
13.439563	1000.276808	12.546061
13.476740	1005.448465	12.551079
13.649568	1004.669153	12.556096
13.271337	1006.392025	12.561114
13.185380	999.186534	12.566131
13.569093	1011.731614	12.571149
13.361196	1027.961545	12.576167
13.787215	1029.650444	12.581184
13.498652	1038.023967	12.586202
13.628129	1028.324217	12.591219
13.727524	1037.741325	12.596237
13.407801	1036.895159	12.601255
13.959652	1023.918501	12.606272
13.635722	1028.490147	12.611290
13.960545	1027.285286	12.616307
13.804312	1028.681251	12.621325
13.493014	1035.155460	12.626343
14.133927	1022.734504	12.631360
13.582850	1028.736627	12.636378
13.982406	1027.480414	12.641395
13.800680	1026.374791	12.646413
13.692849	1027.444249	12.651431
13.890334	1019.913474	12.656448
13.637600	1026.604744	12.661466
14.004861	1027.733316	12.666483
13.900329	1029.861637	12.671501
13.652529	1028.757900	12.676519
13.964145	1018.869338	12.681536
13.651064	1017.844128	12.686554
13.676023	1022.079661	12.691571
13.596900	1027.793792	12.696589
13.661754	1029.288967	12.701607
14.070652	1028.226082	12.706624
13.489935	1031.634000	12.711642
14.214760	1020.876253	12.716659
14.013650	1031.285998	12.721677
13.999612	1032.758018	12.726695
14.010075	1032.813830	12.731712
13.727214	1033.185136	12.736730
13.742581	1034.419224	12.741747
13.864094	1038.060841	12.746765
13.650962	1037.036793	12.751783
14.178333	1044.572077	12.756800
14.110813	1057.893468	12.761818
14.399722	1057.861438	12.766835
14.267132	1049.258185	12.771853
14.130679	1041.726796	12.776871
14.174904	1033.350561	12.781888
13.907293	1038.671124	12.786906
14.123666	1028.664475	12.791923
14.017567	1036.993214	12.796941
14.157438	1053.631313	12.801959
14.152752	1060.698435	12.806976
13.904933	1068.551859	12.811994
14.216386	1061.141950	12.817011
14.399443	1066.226873	12.822029
14.179312	1066.240953	12.827047
14.413124	1065.839321	12.832064
14.381314	1061.718425	12.837082
14.191821	1063.771452	12.842099
14.386477	1065.310093	12.847117
14.449630	1058.862924	12.852135
14.544679	1060.518056	12.857152
14.453345	1051.257206	12.862170
13.887665	1034.749597	12.867187
13.978027	1060.084947	12.872205
14.065718	1063.006212	12.877223
14.237854	1050.522712	12.882240
13.892982	1068.651285	12.887258
14.148837	1069.921534	12.892275
14.575156	1066.694814	12.897293
14.180376	1061.286042	12.902311
14.498882	1062.959680	12.907328
14.450672	1068.382497	12.912346
14.415409	1067.261672	12.917363
14.258376	1072.101352	12.922381
14.323217	1083.819405	12.927399
14.715286	1085.619441	12.932416
14.306083	1091.543370	12.937434
14.586417	1089.519915	12.942451
14.463993	1092.613378	12.947469
14.286048	1096.618369	12.952487
14.668154	1096.298474	12.957504
14.487092	1108.214348	12.962522
14.556769	1097.300483	12.967539
15.071289	1098.487349	12.972557
14.550209	1104.625867	12.977575
14.449288	1086.935762	12.982592
14.589882	1095.146124	12.987610
14.432446	1093.580977	12.992627
14.716724	1082.712684	12.997645
14.327172	1095.207544	13.002663
14.276612	1090.164580	13.007680
14.696969	1099.796675	13.012698
14.571852	1098.681278	13.017715
14.874014	1091.961453	13.022733
14.475713	1101.132683	13.027751
14.314042	1103.435431	13.032768
14.843516	1124.685310	13.037786
14.881029	1127.436557	13.042803
14.851264	1131.374499	13.047821
14.579843	1131.625805	13.052839
14.832337	1135.759125	13.057856
14.595728	1140.971441	13.062874
14.855743	1137.534066	13.067891
14.664589	1124.567771	13.072909
14.915171	1134.466972	13.077927
14.908215	1125.845234	13.082944
14.643531	1132.786551	13.087962
14.697865	1130.774140	13.092979
14.793663	1130.020570	13.097997
14.471282	1141.169346	13.103015
15.058387	1140.778496	13.108032
15.110644	1168.056492	13.113050
15.410050	1163.918513	13.118067
15.400718	1145.506897	13.123085
15.229465	1142.558642	13.128103
14.974529	1136.642449	13.133120
14.995642	1134.909545	13.138138
14.871540	1128.748467	13.143155
15.080425	1138.699062	13.148173
14.694872	1135.887869	13.153191
15.018439	1157.631326	13.158208
15.143168	1163.096795	13.163226
15.470049	1161.648283	13.168243
15.784525	1163.691092	13.173261
14.861473	1158.128830	13.178279
15.090141	1151.493983	13.183296
15.176083	1158.978411	13.188314
15.054454	1165.330716	13.193331
15.309225	1158.682094	13.198349
15.339449	1161.635336	13.203367
15.271266	1160.656565	13.208384
15.376396	1163.300167	13.213402
15.356724	1162.466507	13.218419
15.538578	1156.304751	13.223437
15.409005	1155.882587	13.228455
15.551793	1158.536486	13.233472
15.280709	1157.956660	13.238490
15.296504	1160.137116	13.243507
15.300331	1163.552983	13.248525
15.130235	1174.474602	13.253543
15.307379	1164.926318	13.258560
15.361625	1156.989289	13.263578
15.173632	1170.796460	13.268595
15.417315	1167.556265	13.273613
15.384932	1166.216064	13.278631
15.330481	1164.836212	13.283648
15.325627	1164.507564	13.288666
15.226334	1159.654138	13.293683
15.550131	1162.557976	13.298701
15.471227	1164.432866	13.303719
15.408540	1160.545396	13.308736
15.754203	1166.986061	13.313754
15.420868	1168.266489	13.318771
15.449591	1158.191622	13.323789
15.566295	1186.976257	13.328807
15.664764	1190.785501	13.333824
15.815981	1195.653699	13.338842
15.626141	1197.911520	13.343859
15.904532	1199.472134	13.348877
15.546826	1197.187799	13.353895
15.546992	1196.904775	13.358912
15.858628	1201.338545	13.363930
15.343972	1200.291192	13.368947
16.035473	1197.634295	13.373965
15.488660	1197.484369	13.378983
15.760812	1197.340157	13.384000
15.543937	1200.069765	13.389018
15.513629	1196.860371	13.394035
15.777577	1196.393904	13.399053
15.531427	1194.699741	13.404071
15.614453	1189.704699	13.409088
15.854664	1194.914842	13.414106
15.594628	1204.694321	13.419123
15.868667	1198.821998	13.424141
15.870998	1211.837079	13.429159
16.120268	1226.915949	13.434176
16.207396	1211.560643	13.439194
15.690681	1204.386628	13.444211
15.947266	1200.728553	13.449229
16.039531	1218.081779	13.454247
16.135519	1226.924778	13.459264
16.124521	1213.905740	13.464282
16.077951	1218.119708	13.469299
16.060046	1205.683303	13.474317
15.945096	1201.595822	13.479335
16.154443	1203.513530	13.484352
16.495498	1207.372367	13.489370
16.123169	1196.635956	13.494387
16.178379	1202.541680	13.499405
15.852249	1199.919842	13.504423
16.073133	1199.980571	13.509440
16.408813	1206.563060	13.514458
15.901945	1209.016292	13.519475
16.093430	1218.232438	13.524493
16.004177	1223.669979	13.529511
16.255249	1233.148307	13.534528
16.672702	1225.509355	13.539546
16.427926	1230.339599	13.544563
16.339817	1220.016723	13.549581
16.379709	1212.148183	13.554599
16.182053	1212.219956	13.559616
16.410363	1213.782566	13.564634
16.014961	1225.570644	13.569651
16.561080	1225.116896	13.574669
16.457907	1229.646926	13.579687
16.401673	1232.562925	13.584704
16.421328	1228.575584	13.589722
15.928865	1224.188418	13.594739
16.355064	1226.569812	13.599757
16.232027	1231.546033	13.604775
16.260137	1226.546295	13.609792
16.283132	1229.295240	13.614810
16.095192	1236.005396	13.619827
16.413833	1227.276928	13.624845
16.362244	1226.023365	13.629863
16.148914	1236.451805	13.634880
16.242130	1246.944841	13.639898
16.280009	1261.575691	13.644915
16.436027	1256.299649	13.649933
16.369211	1258.669780	13.654951
16.379134	1260.819728	13.659968
16.712955	1259.061403	13.664986
16.551315	1267.051440	13.670003
16.671376	1266.521400	13.675021
16.712349	1260.841582	13.680039
16.749399	1266.525146	13.685056
16.722526	1266.720210	13.690074
16.538821	1272.114356	13.695091
16.679501	1269.675432	13.700109
16.477819	1274.252496	13.705127
16.417168	1272.062261	13.710144
17.017237	1273.719610	13.715162
16.645016	1269.193230	13.720179
16.592149	1274.020053	13.725197
16.973605	1282.344954	13.730215
17.069756	1300.506666	13.735232
16.978090	1282.181355	13.740250
16.856294	1277.626495	13.745267
16.865160	1275.320419	13.750285
16.918404	1286.437409	13.755303
17.080036	1287.643360	13.760320
16.931576	1285.227906	13.765338
16.950317	1288.683063	13.770355
16.961697	1288.307630	13.775373
17.296972	1287.535261	13.780391
17.004580	1286.716837	13.785408
17.082682	1272.285782	13.790426
16.827447	1266.819184	13.795443
17.052335	1279.306139	13.800461
16.915293	1291.474307	13.805479
16.950249	1292.998079	13.810496
17.079857	1288.842912	13.815514
17.299288	1307.367279	13.820531
17.294340	1297.936074	13.825549
17.112668	1294.191107	13.830567
16.882565	1295.599329	13.835584
17.107460	1291.498458	13.840602
16.916831	1301.007454	13.845619
17.177872	1291.557401	13.850637
17.195431	1296.802875	13.855655
17.022120	1308.129442	13.860672
17.181289	1287.878766	13.865690
17.061685	1287.334477	13.870707
16.988630	1296.288185	13.875725
17.079723	1295.012563	13.880743
17.009345	1298.952942	13.885760
17.611989	1314.246601	13.890778
17.427236	1311.981638	13.895795
17.112045	1310.635109	13.900813
17.482912	1325.123083	13.905831
17.245178	1334.266285	13.910848
17.235685	1333.952181	13.915866
17.344831	1328.279553	13.920883
17.555592	1333.797370	13.925901
17.488988	1341.265023	13.930919
17.388269	1332.511062	13.935936
17.661454	1329.212800	13.940954
17.497178	1335.775776	13.945971
17.823927	1335.808739	13.950989
17.772868	1324.185588	13.956007
17.585219	1342.251042	13.961024
17.776971	1333.847065	13.966042
17.722283	1331.231827	13.971059
17.580021	1331.221200	13.976077
17.716939	1331.932831	13.981095
17.681453	1338.161888	13.986112
17.813485	1335.116523	13.991130
17.718371	1325.203785	13.996147
17.743172	1328.405196	14.001165
17.873456	1329.284457	14.006183
17.909241	1326.045588	14.011200
17.825910	1306.887781	14.016218
17.697325	1302.096246	14.021235
17.586983	1321.632702	14.026253
17.711779	1321.900285	14.031271
17.656340	1336.681697	14.036288
17.918701	1325.870800	14.041306
17.610906	1330.852059	14.046323
17.652911	1334.448646	14.051341
17.869987	1328.486497	14.056359
17.609789	1339.463702	14.061376
17.828707	1328.798184	14.066394
17.764200	1324.479093	14.071411
17.809487	1330.436508	14.076429
17.897773	1326.720055	14.081447
17.691560	1331.144739	14.086464
17.776251	1328.092648	14.091482
18.039438	1338.986331	14.096499
17.918338	1348.361009	14.101517
18.087785	1340.913461	14.106535
18.189007	1350.755646	14.111552
18.468526	1345.513846	14.116570
18.404824	1348.901567	14.121587
18.083770	1340.176216	14.126605
18.442611	1334.309877	14.131623
17.994142	1335.947173	14.136640
17.616253	1337.455067	14.141658
17.894501	1344.020747	14.146675
17.894328	1344.570439	14.151693
17.978360	1345.704600	14.156711
17.875383	1349.618108	14.161728
17.967600	1347.916319	14.166746
17.992610	1353.032627	14.171763
18.076776	1352.371522	14.176781
18.152066	1355.911028	14.181799
18.203634	1375.306961	14.186816
18.193578	1382.222365	14.191834
18.130347	1380.753791	14.196851
18.027660	1391.879356	14.201869
18.295377	1385.069048	14.206887
18.340010	1386.279421	14.211904
18.240612	1384.770380	14.216922
18.352686	1384.864877	14.221939
18.280180	1389.477669	14.226957
18.261346	1378.128271	14.231975
18.115166	1391.387777	14.236992
18.591400	1410.108714	14.242010
18.409260	1410.578700	14.247027
18.757919	1419.822087	14.252045
18.957352	1408.392034	14.257063
18.478628	1409.319790	14.262080
18.919196	1395.360086	14.267098
18.458766	1390.250648	14.272115
18.693410	1380.308070	14.277133
18.661265	1379.881183	14.282151
18.380533	1391.680317	14.287168
18.719147	1397.651780	14.292186
19.135325	1407.574914	14.297203
18.913724	1397.373238	14.302221
18.942671	1387.915893	14.307239
18.784680	1376.345450	14.312256
18.343118	1378.676477	14.317274
18.752206	1391.689309	14.322291
18.869163	1413.400806	14.327309
19.026382	1411.410689	14.332327
18.850654	1416.193730	14.337344
18.770075	1417.734285	14.342362
18.966672	1421.122617	14.347379
18.902331	1418.464475	14.352397
19.197092	1417.549992	14.357415
19.129268	1425.270640	14.362432
19.137031	1411.562906	14.367450
18.748556	1398.181033	14.372467
19.054551	1405.750793	14.377485
19.238564	1406.525493	14.382503
18.737380	1402.584595	14.387520
18.930602	1404.072328	14.392538
19.201646	1406.890856	14.397555
18.986922	1411.136265	14.402573
19.276225	1405.419209	14.407591
19.225117	1409.174932	14.412608
18.978013	1411.467856	14.417626
19.293158	1408.044127	14.422643
18.927938	1414.265220	14.427661
19.153308	1415.824007	14.432679
19.411779	1410.273471	14.437696
19.142773	1412.274751	14.442714
19.252540	1402.793777	14.447731
18.823308	1411.309296	14.452749
19.155224	1406.067854	14.457767
19.066955	1410.332479	14.462784
18.953346	1407.079356	14.467802
19.342922	1405.979490	14.472819
19.024941	1414.911621	14.477837
19.013176	1429.198493	14.482855
19.350804	1436.346892	14.487872
19.486024	1442.501660	14.492890
19.879835	1439.449538	14.497907
19.542315	1452.160473	14.502925
19.832099	1432.006876	14.507943
19.738477	1415.367539	14.512960
19.622200	1407.867276	14.517978
19.894698	1404.338407	14.522995
19.153345	1401.778995	14.528013
19.319037	1402.574052	14.533031
19.454544	1411.483445	14.538048
19.516154	1422.998355	14.543066
19.701253	1429.780677	14.548083
19.467341	1442.374054	14.553101
19.756016	1427.725309	14.558119
19.658962	1429.039856	14.563136
19.851449	1437.382356	14.568154
19.808117	1425.848005	14.573171
19.745862	1434.376387	14.578189
19.824311	1427.710787	14.583207
19.673345	1434.828287	14.588224
19.432663	1430.897785	14.593242
19.797548	1427.356367	14.598259
19.649629	1434.319820	14.603277
19.899773	1426.084075	14.608295
19.766927	1433.802503	14.613312
19.628456	1431.553480	14.618330
19.774531	1432.102184	14.623347
19.872981	1435.624881	14.628365
19.795540	1433.366539	14.633383
19.667957	1436.618797	14.638400
19.612967	1429.996159	14.643418
19.889849	1433.852689	14.648435
20.012334	1460.260917	14.653453
20.539224	1456.122592	14.658471
20.087614	1444.018444	14.663488
19.922248	1439.795550	14.668506
20.017417	1440.318433	14.673523
19.714872	1449.774006	14.678541
20.187723	1448.121376	14.683559
20.376310	1455.677139	14.688576
20.147706	1464.372059	14.693594
20.436423	1465.923510	14.698611
20.447460	1458.734027	14.703629
20.824552	1453.278397	14.708647
20.573049	1433.539234	14.713664
20.161018	1434.479569	14.718682
20.463050	1425.102568	14.723699
20.142717	1428.987523	14.728717
20.055605	1429.903579	14.733735
20.249037	1432.350323	14.738752
20.130152	1431.033479	14.743770
20.412021	1450.292156	14.748787
20.502874	1457.673161	14.753805
20.550718	1454.975569	14.758823
20.640547	1448.603349	14.763840
20.515857	1445.878425	14.768858
20.581118	1433.688691	14.773875
20.288912	1437.042225	14.778893
20.319012	1443.374241	14.783911
20.374396	1446.469432	14.788928
20.139599	1453.707908	14.793946
20.627255	1450.030407	14.798963
20.523386	1449.553585	14.803981
20.560408	1458.150972	14.808999
20.531556	1446.357912	14.814016
20.593099	1453.829988	14.819034
20.734733	1458.559306	14.824051
20.640505	1453.040389	14.829069
20.433866	1452.684915	14.834087
20.535683	1457.164529	14.839104
20.555162	1465.879785	14.844122
20.623102	1450.586476	14.849139
20.632769	1454.082148	14.854157
20.241438	1477.541273	14.859175
21.084794	1478.537104	14.864192
20.723917	1488.692118	14.869210
20.698501	1489.228672	14.874227
21.220601	1491.712336	14.879245
21.009786	1490.988264	14.884263
20.997746	1492.301337	14.889280
20.818209	1488.822896	14.894298
20.791539	1483.288844	14.899315
21.027782	1487.189124	14.904333
20.894239	1491.500639	14.909351
21.123728	1496.387859	14.914368
20.863975	1489.147535	14.919386
21.085004	1490.911378	14.924403
21.163654	1490.638186	14.929421
20.892987	1490.370872	14.934439
21.089479	1484.675062	14.939456
20.721986	1495.607941	14.944474
20.872572	1484.223323	14.949491
21.126210	1487.910882	14.954509
21.111848	1487.322387	14.959527
21.216182	1488.625243	14.964544
21.180916	1502.173561	14.969562
21.382287	1509.491407	14.974579
21.181106	1519.357792	14.979597
21.528178	1517.304334	14.984615
21.362674	1514.245214	14.989632
21.409515	1521.036691	14.994650
21.537820	1510.891169	14.999667
21.607106	1491.327943	15.004685
21.345220	1486.042682	15.009703
21.443818	1482.328028	15.014720
21.404075	1490.224371	15.019738
21.369898	1498.295780	15.024755
21.695494	1505.825728	15.029773
21.540346	1513.538046	15.034791
21.651087	1501.626947	15.039808
21.384908	1505.716337	15.044826
21.608229	1509.747503	15.049843
21.764111	1517.759102	15.054861
21.669269	1517.633536	15.059879
21.693691	1508.017813	15.064896
21.958366	1514.434634	15.069914
21.627338	1491.158986	15.074931
21.710841	1485.446454	15.079949
21.776959	1502.885823	15.084967
21.897131	1494.540857	15.089984
21.591559	1492.636030	15.095002
21.471356	1506.385423	15.100019
21.695487	1513.016042	15.105037
21.628237	1516.677220	15.110055
21.792957	1517.674018	15.115072
21.718808	1512.021047	15.120090
21.571292	1516.777399	15.125107
21.775115	1514.641758	15.130125
21.687365	1506.959560	15.135143
21.656774	1515.654395	15.140160
21.556981	1517.610344	15.145178
21.843521	1535.853400	15.150195
22.422615	1543.176429	15.155213
22.272468	1536.295096	15.160231
22.305470	1515.274864	15.165248
22.167738	1509.669824	15.170266
22.110314	1506.733358	15.175283
22.237249	1507.589957	15.180301
22.007012	1504.408882	15.185319
21.891589	1508.683937	15.190336
21.887995	1519.835703	15.195354
22.222921	1525.666096	15.200371
22.481443	1540.450040	15.205389
22.656911	1545.250159	15.210407
22.636911	1516.218665	15.215424
22.219855	1504.359927	15.220442
22.562784	1510.180721	15.225459
22.644958	1505.525086	15.230477
22.563889	1511.631841	15.235495
22.576327	1508.696404	15.240512
22.173287	1508.441955	15.245530
22.236534	1506.957149	15.250547
22.297747	1503.453010	15.255565
22.167039	1500.277895	15.260583
22.163560	1503.922998	15.265600
22.304072	1518.325679	15.270618
22.538934	1535.479662	15.275635
22.660747	1531.345406	15.280653
22.734654	1538.258393	15.285671
22.778103	1534.888290	15.290688
22.420739	1525.047986	15.295706
22.659712	1533.424965	15.300723
22.664161	1536.217980	15.305741
22.548298	1539.883277	15.310759
22.513845	1533.067431	15.315776
22.694941	1535.717021	15.320794
22.328740	1536.080090	15.325811
22.504273	1529.621203	15.330829
22.594323	1534.076017	15.335847
22.760788	1546.141368	15.340864
22.593221	1535.045618	15.345882
22.874493	1533.535335	15.350899
22.885560	1532.357591	15.355917
22.485367	1538.629800	15.360935
22.821735	1523.145119	15.365952
22.746524	1534.723320	15.370970
22.754819	1551.456575	15.375987
22.930004	1553.816597	15.381005
22.772884	1559.413920	15.386023
22.998896	1562.877726	15.391040
22.772049	1563.803937	15.396058
22.950351	1555.382778	15.401075
23.375411	1557.604571	15.406093
23.162058	1559.766338	15.411111
23.251330	1558.704775	15.416128
23.279923	1566.045354	15.421146
22.894284	1565.885660	15.426163
23.044188	1559.999901	15.431181
22.645986	1576.008375	15.436199
23.091091	1556.146612	15.441216
23.346836	1562.386980	15.446234
23.353181	1566.771413	15.451251
23.364924	1556.917997	15.456269
23.328759	1562.580723	15.461287
23.433331	1561.293398	15.466304
23.394420	1555.175917	15.471322
23.562667	1566.454771	15.476339
23.414139	1563.495192	15.481357
22.993385	1566.802718	15.486375
23.454564	1583.805105	15.491392
23.477241	1592.457303	15.496410
23.691992	1600.869039	15.501427
23.644606	1593.244680	15.506445
23.583843	1595.365435	15.511463
23.521466	1595.149059	15.516480
23.649659	1594.421205	15.521498
23.534313	1596.663991	15.526515
23.607158	1591.159878	15.531533
23.687088	1590.861669	15.536551
23.576588	1585.763509	15.541568
23.442570	1585.689312	15.546586
23.616899	1592.535692	15.551603
23.519285	1581.303128	15.556621
23.847132	1589.255185	15.561639
23.741282	1586.995226	15.566656
24.056423	1595.067893	15.571674
24.061533	1591.438773	15.576691
23.877311	1594.736269	15.581709
23.922253	1594.842279	15.586727
23.575677	1590.015888	15.591744
23.958246	1587.752212	15.596762
23.741444	1590.673214	15.601779
23.939929	1588.977816	15.606797
23.646641	1587.266218	15.611815
23.961503	1595.125546	15.616832
24.147070	1588.770879	15.621850
23.736694	1587.828275	15.626867
24.170082	1598.797498	15.631885
24.136933	1619.659339	15.636903
23.963845	1614.694368	15.641920
24.304049	1621.461325	15.646938
24.237599	1617.532631	15.651955
24.551816	1607.557440	15.656973
24.403631	1622.252513	15.661991
24.474433	1604.219603	15.667008
24.443818	1586.487759	15.672026
24.268262	1583.669266	15.677043
24.438752	1574.970256	15.682061
24.251276	1578.733641	15.687079
24.404193	1582.631997	15.692096
24.799479	1586.608721	15.697114
24.458644	1584.241612	15.702131
24.531416	1575.021778	15.707149
24.516925	1574.308891	15.712167
24.554538	1574.997609	15.717184
24.845748	1576.926611	15.722202
24.762794	1575.047112	15.727219
24.776914	1571.476347	15.732237
24.796031	1587.754701	15.737255
24.482081	1575.898519	15.742272
24.555844	1577.293453	15.747290
24.456248	1581.179293	15.752307
24.222862	1578.618408	15.757325
24.764405	1586.095707	15.762343
24.661315	1600.058096	15.767360
25.134138	1603.251119	15.772378
24.641895	1595.940977	15.777395
24.817545	1597.279671	15.782413
25.046118	1595.911573	15.787431
24.934703	1595.385208	15.792448
24.878317	1582.584795	15.797466
24.678068	1590.714855	15.802483
24.852815	1598.205263	15.807501
25.085699	1600.826603	15.812519
25.307581	1604.495040	15.817536
25.215800	1596.539055	15.822554
24.870136	1584.587330	15.827571
24.964799	1587.475257	15.832589
24.694367	1596.725208	15.837607
24.968476	1594.275949	15.842624
24.959671	1603.759350	15.847642
24.564954	1603.320451	15.852659
24.573359	1599.162043	15.857677
24.934178	1603.392511	15.862695
24.652206	1599.199119	15.867712
24.976611	1622.572222	15.872730
25.226143	1632.491601	15.877747
25.365374	1633.215462	15.882765
25.670586	1635.932311	15.887783
25.611787	1643.047242	15.892800
25.589457	1634.443515	15.897818
25.467050	1636.861492	15.902835
25.550744	1624.803202	15.907853
25.292650	1618.546795	15.912871
25.271651	1629.287742	15.917888
25.373479	1637.263079	15.922906
25.268922	1634.953686	15.927923
25.393688	1633.363011	15.932941
25.487016	1631.895652	15.937959
25.240863	1636.880974	15.942976
25.895087	1630.184507	15.947994
25.501328	1637.855298	15.953011
25.744238	1629.113950	15.958029
25.783679	1630.860636	15.963047
25.940290	1626.932010	15.968064
25.645906	1622.093422	15.973082
25.587922	1626.699155	15.978099
25.556330	1633.403276	15.983117
25.661378	1635.223743	15.988135
25.686590	1628.875535	15.993152
25.718898	1621.980091	15.998170
25.634430	1635.147302	16.003187
25.952964	1631.389498	16.008205
26.142681	1632.141613	16.013223
25.667998	1635.525013	16.018240
25.940998	1642.410588	16.023258
25.761871	1657.434835	16.028275
26.303244	1652.740516	16.033293
26.194876	1649.191198	16.038311
26.139614	1658.919334	16.043328
26.060561	1653.359644	16.048346
26.093627	1658.068812	16.053363
26.089385	1659.363679	16.058381
26.516717	1667.400482	16.063399
26.100436	1659.454501	16.068416
25.865880	1657.706790	16.073434
25.953647	1656.696651	16.078451
26.433361	1649.773562	16.083469
26.259315	1658.372941	16.088487
26.200160	1658.056819	16.093504
26.359459	1645.911583	16.098522
26.441958	1649.055473	16.103539
26.689330	1656.512229	16.108557
26.793738	1650.376095	16.113575
26.533329	1650.492512	16.118592
26.832257	1642.965899	16.123610
26.730898	1654.941434	16.128627
26.692820	1649.790708	16.133645
26.728187	1647.826646	16.138663
26.265773	1658.443861	16.143680
26.687516	1647.530364	16.148698
26.446944	1657.127768	16.153715
26.437525	1649.686859	16.158733
26.701998	1636.652952	16.163751
26.682748	1640.599124	16.168768
26.673116	1647.827568	16.173786
26.385751	1656.585476	16.178803
26.597706	1648.514205	16.183821
26.906550	1647.962340	16.188839
26.760234	1653.126409	16.193856
26.685825	1647.862803	16.198874
26.502067	1647.264951	16.203891
26.509955	1657.601135	16.208909
26.967063	1668.988922	16.213927
26.490928	1682.858436	16.218944
26.838755	1681.910348	16.223962
26.685826	1679.238091	16.228979
26.704818	1689.648835	16.233997
26.753163	1683.325120	16.239015
26.883928	1689.224030	16.244032
27.030786	1689.234029	16.249050
27.037817	1687.159300	16.254067
26.843692	1707.687284	16.259085
27.609512	1706.962891	16.264103
27.280207	1714.855724	16.269120
27.593024	1700.952336	16.274138
27.228207	1695.056879	16.279155
27.354594	1680.489890	16.284173
27.653917	1675.234858	16.289191
27.153622	1676.286673	16.294208
27.389927	1672.454681	16.299226
27.255437	1677.873494	16.304243
27.422202	1700.650770	16.309261
27.684370	1708.010612	16.314279
27.655701	1690.517305	16.319296
27.495330	1675.843869	16.324314
27.489097	1676.648120	16.329331
27.535184	1690.643367	16.334349
28.062760	1696.979327	16.339367
28.145362	1686.259366	16.344384
27.731471	1684.570090	16.349402
27.698141	1666.168130	16.354419
27.744218	1674.757838	16.359437
27.658995	1667.387347	16.364455
27.703373	1674.406465	16.369472
27.592972	1675.530723	16.374490
27.788317	1677.962229	16.379507
27.701915	1678.434873	16.384525
27.674064	1690.629759	16.389543
27.915497	1704.536765	16.394560
27.992080	1704.848560	16.399578
28.208676	1700.270609	16.404595
27.725452	1702.875906	16.409613
27.886983	1704.569311	16.414631
27.739419	1710.028096	16.419648
28.146205	1703.926907	16.424666
28.223419	1705.834276	16.429683
27.920020	1704.445994	16.434701
28.349371	1701.460379	16.439719
28.301732	1706.014028	16.444736
28.183642	1703.162767	16.449754
28.432597	1695.471175	16.454771
27.795053	1695.946897	16.459789
28.572053	1698.695474	16.464807
28.284453	1697.599853	16.469824
28.465500	1697.782144	16.474842
28.519557	1700.660281	16.479859
28.103575	1705.963513	16.484877
28.380286	1701.811829	16.489895
28.106603	1705.776923	16.494912
28.157356	1704.731964	16.499930
27.924164	1699.956448	16.504947
28.481340	1722.983281	16.509965
28.823277	1729.688187	16.514983
28.422986	1731.623057	16.520000
28.618995	1724.122110	16.525018
28.728638	1733.650543	16.530035
28.422621	1732.400488	16.535053
28.601384	1724.564598	16.540071
28.622141	1732.939238	16.545088
28.741091	1719.438412	16.550106
28.698983	1726.133291	16.555123
28.817866	1729.950311	16.560141
28.754876	1728.748201	16.565159
29.160203	1730.281158	16.570176
28.877241	1737.143486	16.575194
29.103807	1718.735434	16.580211
28.853088	1726.804630	16.585229
28.784162	1725.029484	16.590247
29.170583	1729.063226	16.595264
28.747546	1731.981398	16.600282
28.920997	1729.005476	16.605299
28.752961	1726.264452	16.610317
28.970510	1727.576533	16.615335
29.123582	1725.188637	16.620352
28.907355	1724.679230	16.625370
29.088081	1716.101676	16.630387
29.078849	1721.769055	16.635405
29.135351	1722.855441	16.640423
29.363931	1726.904297	16.645440
29.118983	1718.895660	16.650458
29.445346	1729.749235	16.655475
29.238404	1740.678927	16.660493
29.512454	1744.706872	16.665511
29.532643	1743.739020	16.670528
29.520109	1746.118346	16.675546
29.707659	1734.854984	16.680563
29.541230	1730.314467	16.685581
29.585626	1717.221268	16.690599
29.618451	1711.775314	16.695616
29.681940	1717.260569	16.700634
29.665085	1706.099581	16.705651
29.401165	1718.544213	16.710669
29.677582	1731.102921	16.715687
29.743401	1746.131573	16.720704
29.553014	1741.223757	16.725722
29.667871	1740.300859	16.730739
29.771741	1750.287349	16.735757
29.709309	1741.860678	16.740775
29.835037	1744.556087	16.745792
29.792586	1741.246621	16.750810
30.055033	1730.972048	16.755827
29.804457	1736.589241	16.760845
29.882424	1736.718916	16.765863
29.991372	1735.504476	16.770880
29.860761	1744.927818	16.775898
30.073038	1734.781631	16.780915
29.900504	1735.983111	16.785933
30.030297	1731.242752	16.790951
30.288094	1733.433609	16.795968
29.734820	1736.627680	16.800986
30.120309	1736.973363	16.806003
29.827033	1746.706322	16.811021
30.250343	1750.650497	16.816039
30.223573	1762.800772	16.821056
30.298203	1772.770858	16.826074
30.511272	1765.569824	16.831091
30.328755	1772.969083	16.836109
30.710371	1775.677242	16.841127
30.412958	1767.126475	16.846144
30.524956	1769.579672	16.851162
30.506913	1764.363779	16.856179
30.638746	1760.997889	16.861197
30.791267	1757.534479	16.866215
30.692356	1768.985675	16.871232
30.732009	1761.803911	16.876250
30.604838	1744.969380	16.881267
30.307499	1750.653770	16.886285
30.744595	1758.581131	16.891303
30.664350	1759.926387	16.896320
30.635523	1762.759599	16.901338
30.903239	1755.342825	16.906355
30.810214	1764.891847	16.911373
30.915596	1752.500336	16.916391
30.872615	1754.139423	16.921408
30.621283	1763.132370	16.926426
30.929533	1753.926979	16.931443
30.837611	1759.571451	16.936461
30.736684	1755.266145	16.941479
31.103411	1748.969602	16.946496
30.931362	1755.492703	16.951514
30.799660	1746.162925	16.956531
30.594226	1752.253360	16.961549
30.981389	1746.558558	16.966567
30.806668	1760.639253	16.971584
31.172704	1778.027298	16.976602
31.374861	1777.159234	16.981619
31.161892	1788.926580	16.986637
31.431753	1782.725593	16.991655
31.295614	1778.203668	16.996672
31.086858	1782.312361	17.001690
31.726959	1778.235522	17.006707
31.571481	1783.564933	17.011725
31.614562	1780.754687	17.016743
31.676835	1789.040198	17.021760
31.687414	1790.836170	17.026778
31.590319	1777.854539	17.031795
31.733955	1777.969010	17.036813
31.492069	1761.487713	17.041831
31.900503	1760.873682	17.046848
31.535216	1769.706762	17.051866
31.752001	1762.298025	17.056883
31.677469	1784.957508	17.061901
31.868964	1776.011204	17.066919
31.960702	1779.190994	17.071936
31.775816	1771.046398	17.076954
31.815211	1772.545073	17.081971
31.742277	1782.262040	17.086989
31.636557	1771.506669	17.092007
31.729342	1786.173804	17.097024
31.842075	1781.138614	17.102042
31.755120	1776.068776	17.107059
31.805812	1774.162004	17.112077
31.999472	1778.834379	17.117095
32.136851	1784.604669	17.122112
31.889145	1786.825306	17.127130
32.132211	1782.324444	17.132147
31.962644	1779.027752	17.137165
31.896632	1787.822307	17.142183
32.179090	1802.393480	17.147200
32.294248	1816.322285	17.152218
32.216785	1813.133170	17.157235
32.245492	1817.752163	17.162253
32.273331	1815.716491	17.167271
32.298038	1817.468393	17.172288
32.131632	1817.035380	17.177306
32.515230	1813.559676	17.182323
32.436385	1817.563794	17.187341
32.399135	1813.069972	17.192359
32.804604	1806.429979	17.197376
32.537334	1812.464535	17.202394
32.494395	1804.156650	17.207411
32.337901	1809.429545	17.212429
32.429284	1808.364072	17.217447
32.451570	1808.683286	17.222464
32.408245	1831.251054	17.227482
32.838327	1831.958651	17.232499
32.574207	1832.900892	17.237517
32.644276	1843.404857	17.242535
33.002451	1836.999852	17.247552
32.401766	1845.373522	17.252570
32.629722	1834.115209	17.257587
32.650694	1841.844982	17.262605
32.691570	1837.593337	17.267623
32.730242	1843.695748	17.272640
32.949084	1862.826791	17.277658
32.842809	1864.070066	17.282675
32.950673	1862.268778	17.287693
33.233954	1861.885314	17.292711
33.778560	1868.910269	17.297728
33.538896	1870.740603	17.302746
33.366239	1858.730488	17.307763
33.798680	1853.316343	17.312781
33.673754	1838.179790	17.317799
33.512027	1827.784053	17.322816
33.608552	1826.901195	17.327834
33.412752	1815.839052	17.332851
33.638723	1820.344276	17.337869
33.574160	1824.071618	17.342887
33.663573	1821.210384	17.347904
33.606368	1827.182206	17.352922
33.747579	1823.002928	17.357939
33.640323	1827.646013	17.362957
33.677776	1824.117390	17.367975
33.591334	1819.225014	17.372992
33.795906	1823.628269	17.378010
33.745826	1819.761381	17.383027
33.838882	1821.265349	17.388045
33.455870	1827.612388	17.393063
33.943590	1817.200059	17.398080
33.871060	1824.709083	17.403098
34.018061	1826.424200	17.408115
34.108980	1822.557979	17.413133
33.713111	1823.194079	17.418151
34.235224	1821.574201	17.423168
33.890918	1826.349455	17.428186
34.016927	1823.201842	17.433203
34.185282	1821.579914	17.438221
34.103403	1830.180661	17.443239
33.996980	1825.588840	17.448256
34.076293	1842.495690	17.453274
34.326570	1841.741703	17.458291
34.116023	1853.340584	17.463309
33.991356	1863.319321	17.468327
34.211087	1853.683247	17.473344
33.970836	1853.533725	17.478362
34.114314	1853.889959	17.483379
34.324611	1858.548973	17.488397
34.250696	1855.083668	17.493415
34.277231	1858.850263	17.498432
34.264730	1874.571153	17.503450
34.355610	1881.285416	17.508467
34.813937	1884.163966	17.513485
34.805021	1882.654066	17.518503
34.798567	1878.690173	17.523520
34.793164	1887.163719	17.528538
34.796035	1873.536310	17.533555
34.907871	1879.428584	17.538573
34.764590	1891.782115	17.543591
34.757359	1877.516600	17.548608
34.946736	1876.885690	17.553626
35.060461	1875.133825	17.558643
34.986462	1877.853276	17.563661
34.853264	1875.247403	17.568679
35.120151	1871.329195	17.573696
35.172722	1878.056100	17.578714
35.299150	1873.956029	17.583731
35.490406	1870.798389	17.588749
35.185666	1872.059568	17.593767
35.305470	1867.156252	17.598784
35.272673	1870.581096	17.603802
35.202227	1863.452950	17.608819
35.168586	1861.143984	17.613837
35.175600	1875.993914	17.618855
35.405121	1868.425929	17.623872
35.379659	1872.855874	17.628890
35.483305	1873.939582	17.633907
35.528202	1871.885723	17.638925
35.392146	1864.682220	17.643943
35.288760	1874.938942	17.648960
35.479979	1874.707733	17.653978
35.361162	1873.270758	17.658995
35.530117	1868.827027	17.664013
35.480428	1873.932648	17.669031
35.223449	1869.151962	17.674048
35.200436	1874.334270	17.679066
35.588565	1899.397267	17.684083
35.547633	1885.813322	17.689101
35.628152	1902.806654	17.694119
35.774513	1894.652810	17.699136
35.961488	1900.852734	17.704154
35.871512	1893.659697	17.709171
35.909357	1894.321225	17.714189
35.817437	1901.234668	17.719207
35.852029	1894.706842	17.724224
36.139753	1898.121529	17.729242
35.873541	1894.892786	17.734259
36.191017	1897.231267	17.739277
36.143855	1896.912759	17.744295
36.101471	1897.965532	17.749312
35.983961	1916.548393	17.754330
36.419685	1925.938693	17.759347
36.680035	1921.406976	17.764365
36.273892	1924.527113	17.769383
36.410583	1924.966758	17.774400
36.726462	1925.901150	17.779418
36.818539	1917.730692	17.784435
36.757184	1899.058681	17.789453
36.647765	1893.264559	17.794471
36.443693	1892.818095	17.799488
36.652650	1890.265011	17.804506
36.565362	1890.159057	17.809523
36.881777	1896.977714	17.814541
36.678116	1911.849179	17.819559
36.684073	1909.806882	17.824576
36.687813	1912.399291	17.829594
36.446635	1923.214305	17.834611
36.732819	1915.571558	17.839629
36.710009	1923.314921	17.844647
36.825848	1919.000446	17.849664
36.813684	1919.860417	17.854682
36.659669	1921.052939	17.859699
37.223303	1904.365657	17.864717
36.842677	1913.463960	17.869735
36.785050	1908.275047	17.874752
37.093744	1918.502142	17.879770
36.973396	1929.904643	17.884787
37.190072	1944.354164	17.889805
37.294240	1946.881916	17.894823
37.226685	1947.488064	17.899840
37.266348	1944.757095	17.904858
37.607673	1934.560667	17.909875
37.424747	1931.726007	17.914893
37.500241	1938.797180	17.919911
37.350844	1945.108730	17.924928
37.550182	1945.333273	17.929946
37.588685	1944.359620	17.934963
38.050601	1929.376986	17.939981
37.765141	1930.755058	17.944999
38.016705	1933.478876	17.950016
37.833343	1936.088099	17.955034
37.424686	1925.157191	17.960051
37.823408	1929.395253	17.965069
37.750691	1941.649342	17.970087
37.633996	1934.124484	17.975104
37.969953	1932.381875	17.980122
37.591118	1931.110396	17.985139
37.947743	1931.213615	17.990157
37.512763	1932.105807	17.995175
38.025447	1936.817135	18.000192
38.124512	1940.699696	18.005210
37.844650	1937.740138	18.010227
38.106309	1936.968120	18.015245
37.679447	1941.502744	18.020263
37.826474	1950.836140	18.025280
38.187809	1968.357464	18.030298
37.938832	1973.447299	18.035315
38.229576	1960.173727	18.040333
38.293032	1968.904031	18.045351
38.164991	1968.046540	18.050368
38.260614	1959.606176	18.055386
38.097441	1969.571278	18.060403
38.422028	1969.113255	18.065421
38.275557	1977.366503	18.070439
38.037634	1981.332831	18.075456
38.358806	1994.021353	18.080474
38.777801	2005.809806	18.085491
38.508158	2006.817146	18.090509
38.704160	2003.169705	18.095527
38.608271	2003.021867	18.100544
38.979920	2000.771753	18.105562
38.661063	2008.744895	18.110579
38.579564	1993.171067	18.115597
39.056833	2005.950289	18.120615
38.697547	1994.186727	18.125632
39.194211	2003.089019	18.130650
39.065138	2011.127588	18.135667
39.352372	1999.349878	18.140685
39.116365	2000.091799	18.145703
39.042722	1993.978320	18.150720
39.427372	2008.064250	18.155738
39.373258	2009.668987	18.160755
39.608662	1990.007938	18.165773
39.468835	1988.193714	18.170791
39.299322	1979.702753	18.175808
39.539226	1973.630670	18.180826
39.564206	1979.116490	18.185843
39.805692	1970.648816	18.190861
39.948120	1978.344764	18.195879
39.806872	1978.363496	18.200896
39.854175	1972.029600	18.205914
39.816722	1978.044273	18.210931
39.759713	1974.149754	18.215949
39.873751	1973.204537	18.220967
39.626095	1972.782217	18.225984
40.171325	1971.876623	18.231002
39.746099	1978.707496	18.236019
40.195031	1970.014914	18.241037
40.506418	1965.648359	18.246055
39.736415	1971.283144	18.251072
39.830767	1971.147898	18.256090
39.810843	1975.794283	18.261107
40.243358	1979.858256	18.266125
40.322497	1974.712815	18.271143
40.026176	1985.844491	18.276160
39.951777	1973.541632	18.281178
40.008762	1973.264145	18.286195
40.268983	1969.573794	18.291213
39.979507	1973.523065	18.296231
39.664986	1970.140097	18.301248
40.120511	1969.313926	18.306266
39.849830	1976.992454	18.311283
40.281202	1984.064561	18.316301
40.457197	2004.993863	18.321319
40.100265	2002.413993	18.326336
40.510043	1998.519731	18.331354
40.520856	2003.470097	18.336371
40.670213	2004.174976	18.341389
40.583494	2003.842937	18.346407
40.580732	2011.822006	18.351424
40.540577	1997.059065	18.356442
40.425350	2011.540775	18.361459
40.755903	2004.601286	18.366477
40.672313	2011.327173	18.371495
40.839618	2032.349685	18.376512
40.738860	2030.329768	18.381530
40.315556	2040.623827	18.386547
40.373955	2039.160640	18.391565
40.949067	2044.322306	18.396583
40.988892	2037.839224	18.401600
40.977083	2046.132810	18.406618
40.923987	2057.036066	18.411635
40.946434	2066.040939	18.416653
41.661326	2063.177269	18.421671
41.331816	2072.616029	18.426688
41.556603	2060.117096	18.431706
41.713620	2063.886545	18.436723
41.845009	2062.162837	18.441741
42.079122	2053.710906	18.446759
41.878109	2037.777286	18.451776
42.070287	2021.434468	18.456794
41.979604	2022.962189	18.461811
42.012782	2019.534625	18.466829
42.031066	2010.933020	18.471847
41.790687	2026.265016	18.476864
41.739207	2015.267417	18.481882
41.974678	2025.484267	18.486899
41.664125	2017.998163	18.491917
41.925018	2012.335198	18.496935
41.785818	2023.279461	18.501952
41.774597	2015.058733	18.506970
41.945775	2020.968401	18.511987
41.811134	2019.585215	18.517005
41.777370	2016.502604	18.522023
41.865995	2020.900707	18.527040
42.114555	2023.401805	18.532058
42.308647	2043.063562	18.537075
42.133806	2049.017153	18.542093
42.134487	2041.577139	18.547111
42.143067	2057.881747	18.552128
42.263745	2050.703362	18.557146
42.508261	2047.216780	18.562163
42.476834	2049.521326	18.567181
42.364753	2048.393070	18.572199
41.804389	2044.731889	18.577216
42.271035	2039.181698	18.582234
42.336961	2045.446609	18.587251
42.411976	2061.856365	18.592269
42.604902	2080.732908	18.597287
42.564365	2079.303423	18.602304
42.971142	2078.051056	18.607322
42.628604	2075.656591	18.612339
42.798484	2077.476218	18.617357
43.303638	2067.794323	18.622375
42.967833	2072.097363	18.627392
43.261373	2063.528891	18.632410
43.074876	2069.603320	18.637427
42.689875	2075.744089	18.642445
43.012616	2069.805894	18.647463
42.979665	2069.637396	18.652480
43.134374	2063.831362	18.657498
43.081095	2066.719074	18.662515
43.005718	2070.246291	18.667533
43.354339	2062.724240	18.672551
43.183665	2064.593960	18.677568
43.429190	2066.595947	18.682586
43.470026	2065.916791	18.687603
43.500782	2082.740209	18.692621
43.562122	2083.200604	18.697639
43.493942	2084.432076	18.702656
43.786267	2084.083726	18.707674
43.702498	2077.365181	18.712691
43.532028	2083.072384	18.717709
43.882348	2079.993090	18.722727
43.508325	2086.715133	18.727744
43.898282	2078.426364	18.732762
43.491085	2079.291915	18.737779
43.680400	2081.958743	18.742797
44.024209	2078.221847	18.747815
43.922594	2082.918012	18.752832
43.854286	2075.095694	18.757850
43.753123	2087.397916	18.762867
44.020483	2096.496507	18.767885
43.994216	2101.823528	18.772903
44.323689	2111.837068	18.777920
44.628592	2103.595049	18.782938
44.387197	2106.110756	18.787955
44.164445	2108.442662	18.792973
44.288651	2104.850002	18.797991
44.310000	2114.563375	18.803008
44.599067	2114.050992	18.808026
44.652714	2097.787729	18.813043
44.554113	2100.467984	18.818061
44.888872	2101.198468	18.823079
44.671473	2107.535912	18.828096
44.606253	2108.426727	18.833114
44.787703	2106.429755	18.838131
44.701684	2108.859889	18.843149
44.781814	2099.027089	18.848167
44.466057	2103.880773	18.853184
44.649400	2094.870674	18.858202
44.492178	2110.477968	18.863219
44.624558	2126.070394	18.868237
44.962791	2131.740622	18.873255
44.795743	2130.667133	18.878272
45.052355	2128.628578	18.883290
45.307617	2120.664857	18.888307
45.078797	2127.405001	18.893325
45.413924	2119.289075	18.898343
45.205641	2125.524619	18.903360
45.299631	2122.433825	18.908378
45.862167	2117.020489	18.913395
45.255196	2133.892084	18.918413
45.566885	2115.688765	18.923431
45.258703	2129.790713	18.928448
45.553135	2145.706335	18.933466
45.843104	2147.339150	18.938483
45.790726	2158.428191	18.943501
45.960281	2151.496793	18.948519
45.982035	2145.290290	18.953536
45.946329	2122.828202	18.958554
45.991482	2121.666423	18.963571
45.872313	2122.027179	18.968589
46.044664	2108.307717	18.973607
45.803045	2115.944098	18.978624
45.817098	2127.464650	18.983642
46.407214	2133.199473	18.988659
46.024733	2148.903951	18.993677
46.474277	2143.453016	18.998695
46.158991	2141.211513	19.003712
46.216159	2143.848659	19.008730
46.305226	2142.797327	19.013747
46.418042	2153.912949	19.018765
46.596673	2139.609329	19.023783
46.557780	2147.166877	19.028800
46.810945	2144.615487	19.033818
47.000085	2136.391833	19.038835
46.388219	2126.555491	19.043853
46.472418	2121.080807	19.048871
46.324601	2137.422421	19.053888
46.478774	2137.535545	19.058906
46.607022	2142.809434	19.063923
46.427243	2143.164084	19.068941
46.412440	2145.789918	19.073959
46.548271	2142.444152	19.078976
46.289179	2158.695943	19.083994
46.544654	2163.166460	19.089011
46.664496	2178.625971	19.094029
46.884226	2173.481201	19.099047
46.737084	2168.709793	19.104064
46.925859	2197.710361	19.109082
47.089837	2195.404842	19.114099
47.138453	2201.433303	19.119117
47.428004	2201.151555	19.124135
47.155379	2200.916834	19.129152
47.369954	2207.728870	19.134170
47.602509	2202.922925	19.139187
47.492615	2203.896736	19.144205
47.742590	2196.295677	19.149223
47.848914	2206.408044	19.154240
47.612874	2201.441496	19.159258
47.883912	2195.410237	19.164275
47.658038	2201.190440	19.169293
48.036614	2194.533871	19.174311
48.307253	2191.658308	19.179328
47.889681	2199.936881	19.184346
48.009333	2189.854163	19.189363
47.975867	2196.523403	19.194381
48.211372	2185.974242	19.199399
47.996667	2190.455694	19.204416
48.039223	2189.083702	19.209434
48.370484	2191.936107	19.214451
48.369909	2195.646249	19.219469
48.154325	2181.369285	19.224487
48.288207	2187.993486	19.229504
48.299106	2189.305182	19.234522
48.151816	2188.264245	19.239539
48.179642	2184.976119	19.244557
48.223946	2190.522595	19.249575
48.289963	2203.350395	19.254592
48.166229	2212.856349	19.259610
48.425696	2213.515839	19.264627
48.504632	2224.627672	19.269645
48.665113	2218.056423	19.274663
49.147412	2224.214661	19.279680
48.797689	2214.510057	19.284698
48.863436	2209.252579	19.289715
48.802089	2213.838569	19.294733
49.047211	2219.652207	19.299751
48.899947	2207.729352	19.304768
49.013471	2205.977483	19.309786
49.003145	2212.662190	19.314803
49.036949	2211.477086	19.319821
49.251751	2214.121606	19.324839
49.330203	2216.719411	19.329856
48.957066	2214.429207	19.334874
49.210659	2225.903474	19.339891
49.114055	2239.585430	19.344909
49.350777	2238.993913	19.349927
49.551390	2242.728233	19.354944
49.681549	2243.515046	19.359962
49.828488	2241.200531	19.364979
49.940875	2236.388095	19.369997
49.701331	2241.191797	19.375015
49.980713	2238.466753	19.380032
49.969320	2243.579934	19.385050
49.609280	2235.154242	19.390067
49.550524	2244.106914	19.395085
49.520271	2244.312786	19.400103
49.548105	2239.736012	19.405120
49.846351	2244.144744	19.410138
50.292439	2254.788305	19.415155
50.255135	2272.692534	19.420173
50.167582	2264.368168	19.425191
50.207585	2256.662474	19.430208
50.206945	2256.324443	19.435226
50.511619	2257.691832	19.440243
50.329356	2266.587407	19.445261
50.263192	2254.874718	19.450279
50.310548	2255.479566	19.455296
50.494028	2266.360329	19.460314
50.735506	2255.058920	19.465331
50.393401	2261.550547	19.470349
50.595515	2258.868610	19.475367
50.856834	2254.813428	19.480384
50.646693	2249.822891	19.485402
50.664846	2243.652773	19.490419
50.719014	2246.053809	19.495437
50.913753	2260.923417	19.500455
51.049279	2269.525022	19.505472
50.887717	2279.900703	19.510490
51.270334	2275.423838	19.515507
51.062388	2278.906516	19.520525
51.207602	2278.887654	19.525543
51.318380	2273.643959	19.530560
51.299015	2279.675046	19.535578
51.445060	2280.630497	19.540595
51.381314	2281.515566	19.545613
51.091821	2280.359975	19.550631
51.297439	2278.747973	19.555648
50.814483	2285.310966	19.560666
51.060457	2283.460381	19.565683
51.399459	2295.001662	19.570701
51.608055	2307.691760	19.575719
51.756424	2302.575301	19.580736
51.635430	2309.201600	19.585754
51.703234	2306.569062	19.590771
52.135609	2309.296867	19.595789
51.656150	2305.137558	19.600807
52.137473	2305.134302	19.605824
51.671170	2310.379530	19.610842
51.690447	2312.391454	19.615859
51.868429	2303.862853	19.620877
52.105615	2319.156215	19.625895
52.302325	2326.577589	19.630912
52.503297	2337.109033	19.635930
52.430728	2338.287705	19.640947
52.434255	2335.463435	19.645965
52.537149	2339.297822	19.650983
52.652295	2322.335132	19.656000
52.699516	2326.015342	19.661018
52.613620	2324.107103	19.666035
52.234303	2333.401111	19.671053
52.285948	2326.871461	19.676071
52.726268	2322.028319	19.681088
52.593072	2332.791482	19.686106
53.066588	2319.428282	19.691123
53.172220	2318.476956	19.696141
52.885173	2318.712753	19.701159
52.927404	2320.067698	19.706176
52.856671	2314.318982	19.711194
53.156182	2314.906095	19.716211
53.239022	2319.149721	19.721229
53.244425	2316.352704	19.726247
53.461706	2314.292684	19.731264
53.280423	2312.450638	19.736282
53.525643	2310.471823	19.741299
53.654262	2312.002629	19.746317
53.565054	2308.414945	19.751335
53.616767	2306.565421	19.756352
53.348755	2313.038106	19.761370
53.522153	2327.082535	19.766387
53.518730	2339.571536	19.771405
53.400598	2344.092555	19.776423
53.861848	2333.372836	19.781440
53.496506	2347.000564	19.786458
53.915250	2347.427376	19.791475
53.964054	2341.695078	19.796493
53.730184	2335.022144	19.801511
53.900264	2339.744266	19.806528
53.943396	2349.619934	19.811546
54.035377	2362.336081	19.816563
54.441192	2362.265404	19.821581
54.740059	2363.833381	19.826599
54.805803	2351.247948	19.831616
54.673221	2342.264823	19.836634
54.247344	2334.081485	19.841651
54.757845	2339.309861	19.846669
54.857695	2352.858988	19.851687
54.864115	2332.257820	19.856704
55.115829	2327.459688	19.861722
54.538118	2331.202041	19.866739
55.147202	2329.290536	19.871757
54.859944	2332.392246	19.876775
54.612945	2325.200993	19.881792
54.574450	2330.558072	19.886810
54.674900	2339.691138	19.891827
54.979548	2346.849755	19.896845
55.095911	2364.719982	19.901863
55.352144	2352.118754	19.906880
55.429115	2365.574038	19.911898
55.200185	2357.153341	19.916915
55.343076	2350.455022	19.921933
55.185810	2359.737473	19.926951
55.147335	2349.756430	19.931968
55.214656	2351.684810	19.936986
54.914839	2358.506497	19.942003
55.118479	2366.914585	19.947021
55.005369	2386.146521	19.952039
55.447632	2384.748878	19.957056
55.416696	2388.538900	19.962074
55.545193	2389.299223	19.967091
55.790484	2385.623846	19.972109
55.449767	2398.608139	19.977127
56.176432	2405.105139	19.982144
56.238250	2413.458779	19.987162
56.262721	2425.460135	19.992179
56.299310	2409.215121	19.997197
56.471939	2404.977727	20.002215
56.452851	2387.625756	20.007232
56.373806	2382.032336	20.012250
56.299705	2373.411968	20.017267
56.206748	2372.632113	20.022285
56.452089	2395.989161	20.027303
56.639967	2401.174519	20.032320
56.510054	2407.915729	20.037338
56.725745	2407.952523	20.042355
56.352123	2407.966817	20.047373
56.441701	2422.413027	20.052391
56.879341	2411.760160	20.057408
56.684551	2409.969160	20.062426
56.528596	2417.261958	20.067443
56.700843	2407.224724	20.072461
56.601818	2407.985320	20.077479
57.080420	2422.649802	20.082496
57.498387	2423.631105	20.087514
57.248111	2437.662715	20.092531
57.068220	2428.283022	20.097549
56.910744	2430.864416	20.102567
56.895245	2439.965557	20.107584
56.806631	2425.590174	20.112602
56.932894	2432.926803	20.117619
57.287183	2445.560997	20.122637
57.464173	2457.039852	20.127655
57.611573	2451.485292	20.132672
57.457645	2457.300134	20.137690
57.505331	2458.683718	20.142707
57.507825	2447.856412	20.147725
57.683502	2458.136208	20.152743
58.032257	2466.720331	20.157760
58.268621	2473.387137	20.162778
57.988332	2467.835672	20.167795
58.080278	2459.242488	20.172813
57.911466	2483.142681	20.177831
58.258367	2483.375478	20.182848
58.401630	2478.350757	20.187866
58.386521	2480.482183	20.192883
58.556542	2465.847782	20.197901
58.581128	2465.876849	20.202919
58.888364	2467.212730	20.207936
58.978669	2473.224157	20.212954
58.662430	2464.417444	20.217971
59.012072	2469.429574	20.222989
59.025100	2471.981166	20.228007
58.890486	2441.834575	20.233024
58.855793	2433.457268	20.238042
58.837465	2458.643598	20.243059
59.019063	2452.938091	20.248077
58.508978	2461.348268	20.253095
58.971748	2469.712715	20.258112
59.024910	2464.393846	20.263130
58.518137	2464.915647	20.268147
59.000264	2458.620975	20.273165
58.907420	2466.597477	20.278183
58.849205	2489.713577	20.283200
59.405095	2499.858784	20.288218
59.403147	2498.632331	20.293235
59.673461	2495.321311	20.298253
59.766127	2490.421506	20.303271
59.835472	2485.139716	20.308288
60.063056	2498.734358	20.313306
59.589411	2492.748340	20.318323
59.865744	2490.521030	20.323341
59.746973	2486.436597	20.328359
60.054832	2490.020534	20.333376
59.874509	2487.351490	20.338394
59.441762	2490.195023	20.343411
59.600039	2492.719023	20.348429
60.016652	2511.387387	20.353447
59.938602	2519.590613	20.358464
60.238195	2517.840184	20.363482
59.884497	2525.923300	20.368499
59.978754	2512.555017	20.373517
59.885757	2519.167320	20.378535
60.090363	2531.540921	20.383552
60.466483	2554.160761	20.388570
60.219215	2551.829583	20.393587
60.440506	2552.317446	20.398605
60.478652	2554.125478	20.403623
60.445592	2557.304438	20.408640
60.833648	2572.684098	20.413658
61.267360	2578.524915	20.418675
61.426685	2572.128128	20.423693
61.390734	2574.267349	20.428711
61.311105	2565.407618	20.433728
61.791669	2563.088602	20.438746
61.369226	2548.717593	20.443763
61.474548	2543.779060	20.448781
61.398365	2538.628837	20.453799
61.419158	2528.778031	20.458816
61.442997	2524.198686	20.463834
62.028068	2542.762810	20.468851
62.057300	2544.045514	20.473869
61.505407	2538.291739	20.478887
61.677454	2532.072794	20.483904
61.661868	2540.347976	20.488922
61.515989	2557.242104	20.493939
61.831468	2559.809774	20.498957
61.924411	2562.784001	20.503975
61.907398	2564.930715	20.508992
61.865145	2557.164473	20.514010
61.837492	2563.312403	20.519027
61.869350	2567.632260	20.524045
62.008139	2587.566479	20.529063
61.980971	2589.154214	20.534080
62.537619	2588.280561	20.539098
62.475137	2589.795791	20.544115
62.828602	2588.707736	20.549133
62.873268	2595.945348	20.554151
62.541806	2579.258313	20.559168
63.105790	2586.726088	20.564186
62.771396	2591.382601	20.569203
63.018919	2585.618095	20.574221
63.047489	2584.075933	20.579239
62.845708	2580.108377	20.584256
63.338602	2573.782740	20.589274
63.184893	2583.404520	20.594291
62.858711	2589.332586	20.599309
63.350728	2579.872645	20.604327
62.992269	2582.721217	20.609344
63.152706	2585.803571	20.614362
63.133482	2595.127481	20.619379
63.451320	2600.821735	20.624397
63.497728	2607.971263	20.629415
63.286585	2603.518606	20.634432
63.551656	2603.057036	20.639450
63.614602	2613.531598	20.644467
63.521164	2616.026823	20.649485
64.003489	2618.383004	20.654503
63.771399	2616.007962	20.659520
63.779172	2612.809292	20.664538
63.916734	2612.283398	20.669555
64.080214	2632.124210	20.674573
63.908557	2636.408096	20.679591
63.767860	2639.389134	20.684608
64.301070	2632.577633	20.689626
64.076255	2642.778583	20.694643
64.386427	2642.232768	20.699661
64.694610	2632.582356	20.704679
64.528565	2641.119529	20.709696
64.298073	2634.728601	20.714714
64.530679	2635.302001	20.719731
64.518836	2641.733190	20.724749
64.557117	2652.586296	20.729767
64.586678	2661.343075	20.734784
64.891332	2655.445453	20.739802
64.871282	2658.365963	20.744819
64.831995	2658.541050	20.749837
64.747429	2650.782162	20.754855
64.627219	2662.585202	20.759872
65.423773	2672.001256	20.764890
65.219659	2687.192059	20.769907
65.570691	2689.799142	20.774925
65.323780	2686.276857	20.779943
65.271538	2684.394106	20.784960
65.527236	2673.264069	20.789978
65.842088	2680.620771	20.794995
65.707043	2680.775097	20.800013
66.038988	2679.774858	20.805031
65.839508	2679.651252	20.810048
66.129907	2677.494820	20.815066
65.922380	2679.995954	20.820083
65.957005	2668.961192	20.825101
65.964564	2672.784674	20.830119
66.129303	2668.716638	20.835136
66.072022	2657.247072	20.840154
66.144043	2672.789408	20.845171
66.240250	2693.783642	20.850189
66.744436	2698.430863	20.855207
66.452080	2695.831913	20.860224
66.920058	2693.787816	20.865242
67.072859	2690.267457	20.870259
66.953728	2688.952119	20.875277
67.099253	2685.613293	20.880295
66.969344	2677.666610	20.885312
67.164119	2669.230705	20.890330
66.763574	2661.525314	20.895347
66.816178	2679.698607	20.900365
67.054914	2684.385449	20.905383
67.095349	2691.018646	20.910400
66.987523	2689.159666	20.915418
66.911891	2693.056382	20.920435
67.121789	2694.874575	20.925453
67.142928	2685.457107	20.930471
67.186727	2688.907639	20.935488
66.984072	2700.608604	20.940506
67.045480	2715.328273	20.945523
67.056868	2728.977814	20.950541
67.469610	2728.983163	20.955559
67.351717	2749.074274	20.960576
67.846599	2747.729310	20.965594
68.189417	2749.395176	20.970611
68.067813	2749.594131	20.975629
68.151894	2745.909142	20.980647
68.101452	2747.675956	20.985664
68.497679	2744.325135	20.990682
68.399521	2745.036387	20.995699
68.427169	2749.038465	21.000717
68.688619	2745.146140	21.005735
68.648193	2744.814687	21.010752
68.692030	2741.191485	21.015770
68.612092	2742.999406	21.020787
68.526757	2746.927272	21.025805
69.063467	2738.661103	21.030823
68.688847	2737.913695	21.035840
69.002656	2724.534074	21.040858
69.006788	2733.550241	21.045875
69.291015	2739.160342	21.050893
69.115426	2733.448520	21.055911
68.705663	2737.790760	21.060928
69.143474	2734.900412	21.065946
69.032182	2736.695412	21.070963
68.961151	2733.618830	21.075981
69.489060	2750.172839	21.080999
69.221744	2770.223361	21.086016
69.431263	2764.009144	21.091034
69.683105	2765.745592	21.096051
69.138621	2765.949999	21.101069
69.481619	2767.028786	21.106087
69.416525	2772.498696	21.111104
69.728437	2783.682596	21.116122
69.594028	2785.739717	21.121139
69.657837	2784.704731	21.126157
70.086135	2785.070524	21.131175
70.017727	2782.165557	21.136192
70.072635	2783.773975	21.141210
70.150192	2786.467307	21.146227
70.379040	2810.288374	21.151245
70.770275	2812.276570	21.156263
70.558059	2807.202724	21.161280
70.966868	2799.784931	21.166298
71.174887	2801.587306	21.171315
71.047370	2801.491943	21.176333
70.806254	2774.506676	21.181351
70.689139	2779.382402	21.186368
71.020791	2790.959131	21.191386
71.202287	2801.374423	21.196403
70.925336	2801.893219	21.201421
70.901987	2801.200248	21.206439
71.286735	2800.260948	21.211456
71.281586	2794.316535	21.216474
71.289504	2796.002819	21.221491
70.972591	2800.619093	21.226509
71.372238	2794.008787	21.231527
71.420777	2820.895783	21.236544
71.713589	2821.478121	21.241562
71.744252	2820.276167	21.246579
71.708743	2827.481883	21.251597
71.858684	2823.517052	21.256615
71.899655	2822.323234	21.261632
71.885485	2822.712291	21.266650
71.870505	2818.587353	21.271667
71.499812	2828.783444	21.276685
72.142114	2836.274596	21.281703
72.076595	2847.171013	21.286720
72.347849	2851.075687	21.291738
72.534346	2858.700992	21.296755
72.367395	2859.031483	21.301773
72.663022	2849.609806	21.306791
72.851423	2849.884606	21.311808
72.631479	2845.353408	21.316826
72.509525	2852.775041	21.321843
72.697012	2850.287962	21.326861
73.107140	2837.370680	21.331879
72.916912	2842.671556	21.336896
73.081787	2844.147589	21.341914
73.137803	2855.242014	21.346931
73.053801	2873.730303	21.351949
73.393302	2861.779497	21.356967
73.715018	2880.126984	21.361984
73.528236	2879.407131	21.367002
73.923347	2868.995662	21.372019
73.728963	2869.109025	21.377037
73.976087	2868.596479	21.382055
73.801865	2860.168812	21.387072
73.400091	2857.330844	21.392090
73.848314	2855.427806	21.397107
73.900576	2861.366936	21.402125
73.899582	2861.405752	21.407143
73.699637	2869.307667	21.412160
73.880994	2862.396443	21.417178
74.212019	2861.218772	21.422195
73.890119	2869.397988	21.427213
74.211611	2883.620382	21.432231
74.224624	2895.605886	21.437248
73.971732	2904.634788	21.442266
74.154372	2905.188912	21.447283
74.260907	2912.775905	21.452301
74.645477	2913.870655	21.457319
74.754922	2926.457196	21.462336
74.598898	2928.409637	21.467354
74.914586	2923.361735	21.472371
74.633431	2932.314223	21.477389
75.100537	2931.148663	21.482407
75.168249	2936.004070	21.487424
75.349997	2952.582147	21.492442
75.393910	2952.513520	21.497459
75.142849	2952.546496	21.502477
75.487607	2953.208828	21.507495
75.707110	2940.969538	21.512512
75.635391	2944.034889	21.517530
75.953207	2933.692087	21.522547
75.909219	2941.146131	21.527565
75.767005	2930.942503	21.532583
76.165519	2940.418333	21.537600
76.039702	2939.815557	21.542618
76.480624	2934.472482	21.547635
75.939092	2947.074698	21.552653
76.227748	2937.380478	21.557671
76.119617	2940.598720	21.562688
76.216009	2950.319088	21.567706
76.194202	2951.753596	21.572723
76.461035	2964.281820	21.577741
76.469976	2960.271004	21.582759
76.553761	2961.345874	21.587776
76.402833	2958.762833	21.592794
76.754703	2968.907484	21.597811
76.858827	2992.906583	21.602829
76.961420	2994.826840	21.607847
77.045366	2984.177424	21.612864
77.174662	2990.768867	21.617882
77.260187	2979.162416	21.622899
77.237743	2991.288916	21.627917
77.421734	2989.959976	21.632935
77.512517	2983.782264	21.637952
77.164352	2987.733630	21.642970
77.515052	2987.691375	21.647987
77.551607	3011.371347	21.653005
77.914285	3011.999609	21.658023
77.725086	3010.470629	21.663040
77.798049	3022.999109	21.668058
78.119066	3008.770338	21.673075
78.094928	3014.215439	21.678093
77.975674	3010.362858	21.683111
78.325787	3003.560255	21.688128
78.372146	3009.832339	21.693146
78.429254	3014.650546	21.698163
78.433065	3010.598831	21.703181
78.269140	2998.682065	21.708199
78.139145	3003.609604	21.713216
78.599901	3029.619575	21.718234
78.658728	3031.515191	21.723251
78.899860	3042.165280	21.728269
78.653664	3041.037501	21.733287
79.115646	3031.545253	21.738304
78.852154	3036.211023	21.743322
79.265690	3020.225819	21.748339
79.035022	3035.279612	21.753357
79.259966	3034.097445	21.758375
79.388853	3030.627037	21.763392
79.228894	3053.364327	21.768410
79.663353	3067.236264	21.773427
79.502431	3065.598649	21.778445
79.490967	3068.902889	21.783463
79.728082	3062.677685	21.788480
79.943271	3066.071965	21.793498
79.949601	3055.492050	21.798515
79.887259	3056.147381	21.803533
79.987849	3056.162290	21.808551
79.924352	3069.731214	21.813568
80.017932	3086.906766	21.818586
80.369961	3084.542025	21.823603
80.374623	3093.233478	21.828621
80.312322	3098.134088	21.833639
80.666612	3085.645180	21.838656
80.381437	3090.627972	21.843674
80.876376	3084.153749	21.848691
80.820801	3089.705272	21.853709
80.465599	3098.408280	21.858727
80.754220	3102.333768	21.863744
80.565268	3113.341368	21.868762
81.247486	3116.223245	21.873779
81.090100	3109.384934	21.878797
80.970959	3104.721210	21.883815
81.340808	3120.172152	21.888832
81.614800	3136.217385	21.893850
81.937805	3136.849467	21.898867
81.701178	3139.396046	21.903885
81.756481	3145.355649	21.908903
81.576739	3144.960239	21.913920
81.527231	3149.613053	21.918938
82.032852	3141.149835	21.923955
81.931813	3138.401795	21.928973
81.612189	3136.092351	21.933991
82.121607	3133.360170	21.939008
82.009953	3152.913707	21.944026
82.308841	3156.119327	21.949043
82.334329	3162.919783	21.954061
82.250603	3150.364362	21.959079
82.452690	3146.823535	21.964096
82.299453	3165.112194	21.969114
82.413216	3169.411175	21.974131
82.591940	3171.446420	21.979149
82.464521	3186.978587	21.984167
83.010270	3177.842890	21.989184
82.957287	3175.160909	21.994202
83.154075	3190.495287	21.999219
83.250790	3201.964754	22.004237
83.328376	3205.421224	22.009255
83.567564	3207.385432	22.014272
83.707618	3217.620050	22.019290
84.167388	3205.438811	22.024307
84.026367	3201.868161	22.029325
84.151986	3181.826508	22.034343
83.858588	3178.687041	22.039360
83.737218	3173.570077	22.044378
84.012249	3186.930670	22.049395
84.020040	3195.827589	22.054413
83.924280	3204.694016	22.059431
84.185347	3198.865620	22.064448
84.223047	3197.369923	22.069466
84.497321	3195.135770	22.074483
84.437694	3193.269141	22.079501
84.396495	3198.727763	22.084519
84.474570	3181.986442	22.089536
84.535084	3199.189642	22.094554
84.499693	3214.506972	22.099571
84.909050	3221.459661	22.104589
84.947401	3230.141674	22.109607
84.813379	3218.357598	22.114624
85.058859	3225.304743	22.119642
84.998745	3218.275850	22.124659
84.960082	3226.111471	22.129677
85.193160	3246.745956	22.134695
85.472526	3246.206799	22.139712
85.484151	3246.742398	22.144730
85.421191	3245.779953	22.149747
85.934380	3250.108497	22.154765
85.730862	3248.572413	22.159783
85.944893	3248.948500	22.164800
85.755597	3271.792550	22.169818
85.876912	3274.699217	22.174835
86.049320	3276.740641	22.179853
86.052305	3283.828370	22.184871
86.226010	3275.134971	22.189888
86.021859	3280.935203	22.194906
86.587887	3296.749548	22.199923
86.824068	3301.045227	22.204941
86.746460	3298.194449	22.209959
87.275233	3300.766695	22.214976
86.926425	3308.371791	22.219994
87.339605	3298.218887	22.225011
87.577244	3290.418139	22.230029
87.395883	3303.470505	22.235047
87.661094	3292.169538	22.240064
87.679429	3294.817640	22.245082
87.583385	3280.987639	22.250099
87.452656	3261.658874	22.255117
87.210573	3286.176034	22.260135
87.643230	3285.267756	22.265152
87.583588	3283.264097	22.270170
87.500641	3288.501291	22.275187
88.106879	3282.791320	22.280205
87.692304	3288.451969	22.285223
88.091978	3299.244110	22.290240
87.948812	3313.113083	22.295258
87.918357	3321.428546	22.300275
87.791512	3319.977408	22.305293
87.960647	3325.706003	22.310311
88.381371	3329.324605	22.315328
88.072699	3340.066329	22.320346
88.371934	3344.357091	22.325363
88.575416	3346.367391	22.330381
88.789356	3350.237190	22.335399
88.702778	3344.388737	22.340416
88.565456	3361.203961	22.345434
88.543605	3370.198417	22.350451
89.065695	3364.882707	22.355469
88.890522	3376.052402	22.360487
89.023992	3371.390081	22.365504
89.495471	3391.407658	22.370522
89.621055	3396.461918	22.375539
90.276156	3397.905263	22.380557
90.034411	3396.707027	22.385575
90.465794	3391.678800	22.390592
90.156070	3374.823513	22.395610
89.878875	3361.470729	22.400627
90.528094	3379.003862	22.405645
90.026075	3391.794793	22.410663
90.307980	3397.946131	22.415680
90.355628	3392.385313	22.420698
90.455405	3389.494515	22.425715
90.645448	3388.109417	22.430733
90.407186	3385.938448	22.435751
90.630435	3385.433778	22.440768
90.692581	3387.570254	22.445786
90.449873	3388.785445	22.450803
90.807316	3402.332995	22.455821
90.622555	3417.660294	22.460839
91.065035	3422.774307	22.465856
90.974568	3429.516117	22.470874
90.938876	3424.234866	22.475891
91.250859	3435.214083	22.480909
90.952886	3451.267723	22.485927
91.435872	3443.651105	22.490944
91.657349	3449.663239	22.495962
91.854978	3470.914592	22.500979
92.008706	3469.531956	22.505997
91.915513	3478.490250	22.511015
91.908586	3476.673136	22.516032
92.120487	3479.651073	22.521050
91.729084	3481.605938	22.526067
92.117069	3465.468195	22.531085
92.137771	3491.484473	22.536103
92.166674	3492.315287	22.541120
92.223239	3501.153903	22.546138
92.425650	3502.402892	22.551155
92.386902	3504.941570	22.556173
92.632081	3529.426466	22.561191
93.010466	3535.651265	22.566208
93.290995	3527.468843	22.571226
93.316690	3535.235687	22.576243
93.657753	3531.505206	22.581261
93.536394	3529.870046	22.586279
93.580301	3528.062621	22.591296
93.564667	3525.084990	22.596314
93.476968	3530.342740	22.601331
93.825043	3527.152897	22.606349
93.796269	3550.304673	22.611367
94.199512	3543.271360	22.616384
94.074311	3550.166629	22.621402
93.888241	3548.174027	22.626419
94.142555	3542.235585	22.631437
93.937329	3539.284226	22.636455
94.110876	3541.049084	22.641472
94.537381	3548.531037	22.646490
94.430913	3566.913614	22.651507
94.599212	3574.398959	22.656525
94.569078	3571.380801	22.661543
94.714111	3571.852584	22.666560
94.743593	3568.618230	22.671578
94.669882	3579.633850	22.676595
95.113361	3586.759029	22.681613
94.665285	3596.264009	22.686631
95.016847	3598.161229	22.691648
95.396910	3588.616061	22.696666
95.366553	3601.087301	22.701683
95.480549	3600.579846	22.706701
95.625338	3628.535897	22.711719
95.896946	3627.338873	22.716736
96.079259	3633.527664	22.721754
96.030940	3620.104868	22.726771
96.454635	3626.428908	22.731789
96.432622	3627.852487	22.736807
96.411566	3626.391284	22.741824
96.638601	3618.727187	22.746842
96.627016	3623.010823	22.751859
96.679732	3616.790734	22.756877
96.671244	3627.386086	22.761895
96.552902	3621.812902	22.766912
96.712910	3615.866030	22.771930
96.543466	3622.810001	22.776947
96.861869	3624.237063	22.781965
96.925407	3641.970239	22.786983
97.095384	3641.492102	22.792000
97.291387	3644.804243	22.797018
96.888685	3642.809304	22.802035
97.067391	3653.189008	22.807053
97.040308	3669.949691	22.812071
97.146096	3673.905992	22.817088
97.813804	3674.951950	22.822106
97.883306	3695.132160	22.827123
98.207999	3701.547436	22.832141
98.339376	3705.968862	22.837159
98.281276	3705.450131	22.842176
98.533661	3711.854547	22.847194
98.514416	3706.053085	22.852211
98.874131	3703.424742	22.857229
98.758062	3701.103950	22.862247
98.682245	3700.316858	22.867264
98.786011	3697.928954	22.872282
98.654535	3705.554561	22.877299
98.789353	3693.757505	22.882317
99.457654	3701.251470	22.887335
99.174932	3723.203258	22.892352
99.273728	3731.058109	22.897370
99.339299	3725.776526	22.902387
99.515192	3723.196730	22.907405
99.553190	3729.548450	22.912423
99.652841	3731.323203	22.917440
99.975390	3720.895626	22.922458
99.894470	3716.832951	22.927475
99.773148	3716.887756	22.932493
99.746876	3732.739194	22.937511
99.551587	3745.183914	22.942528
100.160275	3740.291990	22.947546
100.120529	3752.473920	22.952563
100.267109	3761.614357	22.957581
100.583093	3779.796902	22.962599
100.422900	3781.170530	22.967616
100.552867	3769.229318	22.972634
100.423673	3783.124742	22.977651
100.649267	3792.964813	22.982669
101.210353	3802.147679	22.987687
101.044709	3804.122689	22.992704
101.087344	3807.596893	22.997722
101.366690	3804.416801	23.002739
101.209820	3799.318503	23.007757
101.717563	3815.482052	23.012775
101.819692	3833.918998	23.017792
102.082819	3830.595503	23.022810
101.862902	3834.257300	23.027827
101.927870	3828.932864	23.032845
102.033553	3823.963155	23.037863
102.170938	3832.842522	23.042880
102.367879	3815.283485	23.047898
102.661479	3824.004679	23.052915
102.297919	3816.273686	23.057933
102.619754	3816.982775	23.062951
102.477383	3822.771008	23.067968
102.610303	3821.191365	23.072986
102.652768	3835.608490	23.078003
102.883528	3843.047002	23.083021
103.005764	3846.810833	23.088039
102.680780	3850.328197	23.093056
102.963627	3844.080937	23.098074
102.926370	3867.962643	23.103091
103.131190	3872.120739	23.108109
103.475498	3890.460163	23.113127
103.442933	3883.307495	23.118144
103.622499	3884.261436	23.123162
103.637523	3905.008497	23.128179
103.846614	3910.511763	23.133197
104.042138	3906.905701	23.138215
103.916550	3907.358909	23.143232
104.139880	3902.772511	23.148250
104.562894	3923.877302	23.153267
104.714013	3931.089638	23.158285
104.658956	3928.509460	23.163303
104.568530	3937.092699	23.168320
104.947048	3919.392835	23.173338
104.965284	3928.892860	23.178355
104.934069	3919.376216	23.183373
105.325044	3923.156207	23.188391
104.932642	3922.431366	23.193408
105.465858	3935.266316	23.198426
105.429800	3939.626543	23.203443
105.611051	3941.379540	23.208461
105.657489	3948.662768	23.213479
105.594580	3945.378271	23.218496
105.654917	3953.134073	23.223514
105.782537	3970.593585	23.228531
105.762018	3978.523442	23.233549
105.970687	3975.738936	23.238567
106.010926	3986.672578	23.243584
106.417929	3991.689490	23.248602
106.307266	3999.831951	23.253619
106.849177	4008.590097	23.258637
106.824920	4011.817509	23.263655
106.954109	4011.110252	23.268672
107.129094	4006.250684	23.273690
107.017436	4000.109242	23.278707
107.178483	3998.503661	23.283725
107.212327	4001.104821	23.288743
107.424064	4008.187451	23.293760
107.731288	4026.105551	23.298778
107.602933	4027.238852	23.303795
107.850601	4035.866967	23.308813
108.005617	4032.714898	23.313831
107.710595	4032.131432	23.318848
108.088341	4030.923105	23.323866
108.067877	4031.113990	23.328883
108.077780	4029.634236	23.333901
108.231140	4033.139376	23.338919
108.147451	4052.725630	23.343936
108.705781	4054.798941	23.348954
108.881375	4056.674955	23.353971
108.755201	4055.778447	23.358989
109.067270	4055.193687	23.364007
108.851623	4054.286005	23.369024
108.784956	4047.921313	23.374042
109.235806	4058.131010	23.379059
108.871033	4071.355742	23.384077
109.286635	4082.177685	23.389095
109.148122	4088.490656	23.394112
109.436720	4083.435059	23.399130
109.431136	4083.888877	23.404147
109.411016	4096.159571	23.409165
109.689928	4101.792311	23.414183
109.646282	4126.580730	23.419200
109.748574	4119.259538	23.424218
110.147318	4125.321335	23.429235
109.907231	4140.387984	23.434253
110.622736	4145.014440	23.439271
110.464326	4150.529813	23.444288
110.638788	4149.977285	23.449306
110.747440	4144.982177	23.454323
110.794888	4159.030999	23.459341
111.028316	4168.665645	23.464359
110.805715	4175.101253	23.469376
111.017427	4166.598738	23.474394
110.794352	4171.678297	23.479411
111.057579	4193.105232	23.484429
111.446717	4200.807503	23.489447
111.352575	4205.285313	23.494464
111.772693	4203.054042	23.499482
111.753321	4209.563905	23.504499
111.951580	4226.391431	23.509517
112.249843	4214.993764	23.514535
112.249605	4219.787581	23.519552
112.186727	4215.654849	23.524570
112.626793	4222.120935	23.529587
112.891545	4246.665534	23.534605
113.083332	4241.718845	23.539623
113.240974	4257.245036	23.544640
113.587269	4239.747819	23.549658
113.334966	4225.943249	23.554675
113.078919	4221.321940	23.559693
113.507711	4224.297186	23.564711
113.604246	4246.755113	23.569728
113.539874	4238.664476	23.574746
113.448104	4242.577242	23.579763
113.394920	4246.565524	23.584781
113.588064	4237.172195	23.589799
113.614657	4256.182869	23.594816
113.870244	4259.045831	23.599834
113.975808	4271.335228	23.604851
113.873534	4267.875260	23.609869
114.047520	4285.914160	23.614887
113.985799	4299.804775	23.619904
114.340132	4303.468071	23.624922
114.593613	4310.481712	23.629939
114.725624	4323.213304	23.634957
114.979679	4325.529981	23.639975
115.075099	4330.538742	23.644992
115.014168	4325.688211	23.650010
115.147285	4319.198975	23.655027
115.510551	4339.317198	23.660045
115.634940	4344.140032	23.665063
116.069151	4354.386543	23.670080
115.867086	4356.492870	23.675098
116.183855	4350.722163	23.680115
116.063571	4348.388978	23.685133
116.436685	4343.222437	23.690151
116.637195	4338.304201	23.695168
116.466549	4338.264793	23.700186
116.502727	4340.841209	23.705203
116.570490	4338.628097	23.710221
116.585502	4335.947259	23.715239
116.602339	4339.595566	23.720256
116.901270	4351.282831	23.725274
117.198232	4357.342672	23.730291
117.195674	4366.290402	23.735309
117.370088	4350.189479	23.740327
117.345296	4355.978915	23.745344
116.980810	4353.589296	23.750362
117.142976	4358.597252	23.755379
117.195941	4390.609158	23.760397
117.356152	4380.555725	23.765415
117.598821	4389.443176	23.770432
117.847428	4403.210833	23.775450
117.967906	4414.598500	23.780467
117.819141	4424.791163	23.785485
117.889963	4428.790460	23.790503
118.112795	4444.924264	23.795520
118.388660	4454.878103	23.800538
118.583999	4449.025873	23.805555
118.795387	4455.544096	23.810573
118.834614	4472.163529	23.815591
119.042878	4474.483085	23.820608
119.368070	4477.173904	23.825626
119.205403	4470.465027	23.830643
119.446656	4473.525714	23.835661
119.687253	4493.851094	23.840679
119.765436	4497.066369	23.845696
119.847594	4502.075017	23.850714
120.329231	4494.874339	23.855731
120.189550	4493.693375	23.860749
120.042016	4487.980594	23.865767
120.432717	4498.450191	23.870784
120.468272	4493.995519	23.875802
120.810701	4512.525784	23.880819
120.810779	4526.890708	23.885837
120.692550	4518.567068	23.890855
120.532660	4529.023893	23.895872
120.645173	4518.187571	23.900890
121.209487	4536.142442	23.905907
121.102104	4549.668327	23.910925
121.314528	4552.707027	23.915943
121.520190	4559.452267	23.920960
121.566890	4555.977020	23.925978
121.546313	4563.035364	23.930995
121.750712	4575.364551	23.936013
121.995419	4577.185082	23.941031
122.424357	4580.771513	23.946048
122.073315	4580.645415	23.951066
122.475980	4574.111445	23.956083
122.203771	4596.986900	23.961101
122.602841	4602.281755	23.966119
122.362432	4602.815422	23.971136
122.335619	4605.445626	23.976154
122.508340	4615.525328	23.981171
122.825563	4635.245965	23.986189
123.203528	4625.462679	23.991207
123.111550	4638.616728	23.996224
123.402605	4658.109398	24.001242
123.820299	4669.644140	24.006259
123.814959	4667.015443	24.011277
123.790760	4664.089024	24.016295
123.962639	4667.313234	24.021312
123.774428	4668.354109	24.026330
124.493785	4679.835761	24.031347
124.561928	4691.726879	24.036365
124.646717	4687.169494	24.041383
124.776223	4687.598600	24.046400
124.691257	4682.629080	24.051418
124.880015	4675.433498	24.056435
124.915209	4676.631122	24.061453
124.737805	4680.438466	24.066471
124.956926	4694.075014	24.071488
125.170164	4697.802719	24.076506
125.343947	4713.456636	24.081523
125.446694	4715.029768	24.086541
125.713310	4707.751188	24.091559
125.748961	4706.979846	24.096576
125.654721	4726.270989	24.101594
126.309589	4733.863371	24.106611
126.179696	4740.813885	24.111629
126.651446	4736.338902	24.116647
126.536249	4724.053231	24.121664
126.521948	4739.308308	24.126682
126.482340	4728.144203	24.131699
127.293131	4757.753762	24.136717
127.252730	4766.932440	24.141735
127.096203	4760.958791	24.146752
126.671036	4764.497668	24.151770
127.075665	4762.820178	24.156787
127.251666	4769.374318	24.161805
127.459185	4786.238715	24.166823
127.369919	4785.866868	24.171840
127.330324	4793.824709	24.176858
127.797657	4789.984429	24.181875
127.762118	4810.460686	24.186893
128.079725	4812.227435	24.191911
128.253023	4811.551431	24.196928
127.929650	4825.157418	24.201946
128.425110	4841.233889	24.206963
128.631374	4844.049210	24.211981
128.592452	4850.189270	24.216999
128.669838	4856.532956	24.222016
128.680750	4876.817318	24.227034
129.139941	4860.912869	24.232051
129.160299	4874.540742	24.237069
129.281165	4882.004246	24.242087
129.842531	4888.198505	24.247104
129.649233	4902.520971	24.252122
130.150493	4894.663971	24.257139
129.975923	4888.903541	24.262157
129.712177	4905.638177	24.267175
130.820371	4916.325548	24.272192
130.584842	4922.370603	24.277210
130.921418	4922.841037	24.282227
131.125520	4927.342127	24.287245
131.142794	4916.930835	24.292263
131.174999	4916.916906	24.297280
130.766508	4917.984030	24.302298
131.217185	4918.178038	24.307315
131.358839	4932.751436	24.312333
131.368908	4945.220199	24.317351
131.786610	4935.559305	24.322368
131.801746	4954.866483	24.327386
132.046021	4944.921633	24.332403
131.984852	4951.108732	24.337421
132.002910	4949.877988	24.342439
132.010756	4961.567438	24.347456
131.947050	4987.072497	24.352474
132.232576	4976.362366	24.357491
132.470550	4989.684959	24.362509
132.736920	4998.267980	24.367527
133.124170	5007.950131	24.372544
132.796316	5000.893493	24.377562
132.995672	5006.686222	24.382579
133.318968	5013.248367	24.387597
133.079333	5040.503487	24.392615
133.728933	5031.396394	24.397632
133.431884	5036.527068	24.402650
133.231526	5030.592076	24.407667
133.918001	5039.155179	24.412685
133.874952	5071.008737	24.417703
133.877875	5069.418992	24.422720
134.092172	5068.369968	24.427738
134.218397	5069.474580	24.432755
134.267159	5080.906107	24.437773
134.267312	5091.488808	24.442791
134.824566	5090.380635	24.447808
134.961888	5105.620414	24.452826
135.242242	5109.613544	24.457843
135.221996	5118.561480	24.462861
135.401346	5117.181943	24.467879
135.686705	5111.041275	24.472896
135.659638	5124.102285	24.477914
135.715961	5117.219835	24.482931
136.208516	5128.481045	24.487949
136.041522	5142.978154	24.492967
136.361498	5140.860998	24.497984
136.434078	5145.557981	24.503002
136.199711	5141.055672	24.508019
136.704047	5153.931849	24.513037
136.871950	5174.526110	24.518055
136.746780	5175.106083	24.523072
137.050114	5178.264530	24.528090
137.040114	5172.646077	24.533107
137.119984	5182.251642	24.538125
137.151009	5201.734485	24.543143
137.301131	5193.115604	24.548160
137.582135	5204.904135	24.553178
137.997250	5214.818075	24.558195
138.148767	5216.052399	24.563213
138.098489	5226.474211	24.568231
138.276930	5225.359443	24.573248
137.834298	5229.314793	24.578266
138.247794	5242.162767	24.583283
138.547149	5246.088993	24.588301
138.408634	5261.304497	24.593319
138.914108	5271.508308	24.598336
138.890360	5285.921974	24.603354
139.162459	5274.196305	24.608371
139.709160	5272.032141	24.613389
139.629561	5272.797530	24.618407
140.023080	5277.313826	24.623424
140.343963	5293.136923	24.628442
140.137064	5294.227399	24.633459
140.575093	5292.565592	24.638477
140.725829	5297.538725	24.643495
140.933315	5299.004790	24.648512
140.817924	5288.753046	24.653530
141.093347	5288.106582	24.658547
141.007096	5284.752423	24.663565
140.791925	5296.780692	24.668583
140.971987	5283.165082	24.673600
141.151576	5290.526122	24.678618
141.342400	5312.932156	24.683635
141.581301	5310.671671	24.688653
141.572818	5325.246664	24.693671
142.001870	5314.857505	24.698688
141.576832	5317.027653	24.703706
141.965823	5332.877318	24.708723
142.435570	5333.737626	24.713741
142.371458	5344.058631	24.718759
142.571095	5342.265382	24.723776
142.182594	5340.123736	24.728794
142.711754	5351.947687	24.733811
142.882511	5363.600223	24.738829
142.751598	5373.673979	24.743847
143.039799	5378.559795	24.748864
142.992924	5379.196907	24.753882
142.900315	5395.365013	24.758899
143.267999	5408.246699	24.763917
143.142677	5411.921943	24.768935
143.639507	5411.793281	24.773952
143.723331	5432.643592	24.778970
143.677413	5432.308658	24.783987
143.838831	5441.362165	24.789005
143.875147	5463.679006	24.794023
144.035466	5468.495450	24.799040
144.011993	5480.099109	24.804058
144.385596	5498.373345	24.809075
144.815502	5503.453115	24.814093
145.184351	5525.584245	24.819111
145.233281	5521.610655	24.824128
145.526374	5524.674781	24.829146
145.427625	5523.821688	24.834163
145.741479	5535.154522	24.839181
145.710680	5543.019923	24.844199
146.153875	5545.359813	24.849216
146.269384	5549.152734	24.854234
146.463159	5548.590663	24.859251
146.848056	5562.844774	24.864269
146.889841	5577.035992	24.869287
146.659395	5569.760555	24.874304
147.017438	5581.787859	24.879322
147.027279	5575.140521	24.884339
147.169404	5574.185324	24.889357
147.415625	5587.967806	24.894375
147.468800	5600.378755	24.899392
147.766586	5597.135005	24.904410
147.525894	5606.977415	24.909427
147.594279	5606.393572	24.914445
148.060808	5626.670409	24.919463
148.228457	5628.842493	24.924480
148.534299	5630.784557	24.929498
148.796739	5636.270148	24.934515
148.650925	5638.122384	24.939533
148.795620	5654.653143	24.944551
148.729222	5648.492535	24.949568
149.206583	5640.238237	24.954586
149.198116	5673.934217	24.959603
149.755426	5673.134740	24.964621
149.337187	5678.692877	24.969639
149.745077	5679.179096	24.974656
149.714558	5692.362439	24.979674
149.690007	5707.194054	24.984691
150.043650	5706.274714	24.989709
149.966238	5712.972019	24.994727
150.512696	5731.012341	24.999744
150.823990	5734.592529	25.004762
150.729928	5743.225396	25.009779
151.004378	5739.612154	25.014797
150.922031	5748.840879	25.019815
150.827829	5765.183688	25.024832
151.255715	5772.072233	25.029850
151.199654	5774.976837	25.034867
151.541593	5793.231455	25.039885
151.451205	5804.432935	25.044903
151.505911	5811.173779	25.049920
151.799607	5821.000304	25.054938
151.928065	5824.644652	25.059955
152.246176	5826.036531	25.064973
152.215645	5847.055969	25.069991
152.480460	5854.215710	25.075008
152.738960	5861.212676	25.080026
152.861379	5866.349775	25.085043
153.054428	5871.365704	25.090061
153.089100	5887.403761	25.095079
153.563808	5879.996465	25.100096
153.460879	5889.138891	25.105114
153.699409	5887.147752	25.110131
153.880687	5905.214081	25.115149
154.067631	5915.013445	25.120167
154.429167	5915.550667	25.125184
154.625114	5911.871623	25.130202
154.452908	5911.584366	25.135219
155.085287	5922.472509	25.140237
155.152346	5932.038120	25.145255
154.672259	5936.357423	25.150272
155.268587	5929.594718	25.155290
155.349302	5940.966445	25.160307
155.388643	5941.316001	25.165325
155.215190	5961.583449	25.170343
155.671390	5960.529761	25.175360
155.918713	5964.047344	25.180378
155.861373	5981.970541	25.185395
156.266754	5988.195793	25.190413
156.203919	6002.798524	25.195431
156.013882	6004.955058	25.200448
156.500856	6011.681915	25.205466
156.710199	6029.510604	25.210483
156.902641	6031.303731	25.215501
156.857430	6044.889912	25.220519
157.000774	6056.459285	25.225536
157.449277	6060.055425	25.230554
157.540031	6087.646733	25.235571
158.034774	6078.621396	25.240589
157.912018	6089.241655	25.245607
158.309948	6082.193533	25.250624
158.350089	6087.553836	25.255642
158.454973	6102.673141	25.260659
158.410035	6105.794136	25.265677
158.393512	6109.097883	25.270695
158.372974	6122.314587	25.275712
158.762953	6122.847895	25.280730
159.132724	6135.494331	25.285747
159.237265	6154.165159	25.290765
159.437588	6164.605169	25.295783
159.450757	6171.743708	25.300800
159.628637	6184.596808	25.305818
159.627777	6202.142291	25.310835
159.913656	6201.017545	25.315853
160.516816	6208.345117	25.320871
160.355831	6218.169982	25.325888
160.634845	6214.845727	25.330906
160.621170	6236.649735	25.335923
160.683227	6247.096939	25.340941
160.872841	6249.194586	25.345959
160.966951	6265.802096	25.350976
161.360443	6265.649586	25.355994
160.963747	6289.898890	25.361011
161.714260	6300.850439	25.366029
161.859588	6305.430968	25.371047
162.405947	6315.066319	25.376064
162.389764	6302.857541	25.381082
162.444401	6322.474117	25.386099
162.921359	6324.621080	25.391117
162.859162	6333.945263	25.396135
163.019941	6336.496650	25.401152
163.202084	6329.655064	25.406170
163.245681	6342.546278	25.411187
163.359036	6351.376700	25.416205
163.260719	6365.806846	25.421223
163.678433	6361.831061	25.426240
163.759093	6361.005716	25.431258
163.891878	6379.009727	25.436275
164.377110	6395.910994	25.441293
164.406311	6388.652051	25.446311
164.656799	6398.242709	25.451328
165.054891	6391.931658	25.456346
165.197430	6397.552362	25.461363
165.064090	6417.179699	25.466381
165.256570	6428.664021	25.471399
165.284065	6432.605627	25.476416
165.672809	6414.771324	25.481434
165.170116	6424.097603	25.486451
165.563626	6436.856134	25.491469
165.923667	6443.206433	25.496487
165.900136	6456.330181	25.501504
166.254156	6470.847787	25.506522
166.431762	6485.563958	25.511539
166.434058	6488.754397	25.516557
166.521270	6505.288474	25.521575
166.834267	6514.152095	25.526592
166.935999	6516.504561	25.531610
167.158724	6540.564264	25.536627
166.924330	6543.695446	25.541645
167.529961	6540.455674	25.546663
167.577007	6556.578213	25.551680
168.134878	6562.042783	25.556698
167.850131	6564.876697	25.561715
168.809152	6580.982959	25.566733
168.702155	6579.522320	25.571751
168.711135	6592.369847	25.576768
168.959232	6585.170666	25.581786
168.806133	6595.641907	25.586803
169.023786	6610.157801	25.591821
169.400852	6613.220842	25.596839
169.414222	6630.269009	25.601856
169.772321	6634.946733	25.606874
169.661005	6641.942262	25.611891
170.178828	6645.071010	25.616909
170.407564	6654.126671	25.621927
170.252763	6673.396344	25.626944
170.454513	6670.525087	25.631962
170.489016	6678.529106	25.636979
171.015455	6695.731845	25.641997
170.842441	6703.664688	25.647015
171.059197	6714.277200	25.652032
171.026196	6723.239969	25.657050
171.152106	6738.587184	25.662067
171.173978	6740.997014	25.667085
171.501556	6755.864254	25.672103
171.837325	6774.278560	25.677120
171.991849	6789.034279	25.682138
172.316959	6803.654647	25.687156
172.324719	6811.172447	25.692173
172.866577	6825.126032	25.697191
172.873211	6830.839493	25.702208
172.987528	6831.362545	25.707226
173.112275	6847.993948	25.712244
173.011953	6862.104298	25.717261
173.476344	6869.456731	25.722279
173.820398	6889.046570	25.727296
174.141266	6893.984164	25.732314
174.384943	6901.472400	25.737332
174.443452	6903.261809	25.742349
174.469858	6908.536445	25.747367
174.713650	6921.754948	25.752384
175.114698	6921.373550	25.757402
175.012962	6925.017668	25.762420
175.409445	6922.299228	25.767437
175.632188	6916.351761	25.772455
175.638468	6940.471536	25.777472
176.081605	6945.891436	25.782490
176.307063	6943.012267	25.787508
176.048247	6943.874358	25.792525
176.187879	6930.935124	25.797543
176.474681	6952.869957	25.802560
176.733982	6964.932781	25.807578
176.921848	6971.781251	25.812596
176.910510	6983.822733	25.817613
177.021917	6972.642280	25.822631
176.829777	6986.726195	25.827648
177.079076	7000.859914	25.832666
177.277029	7014.286152	25.837684
177.593080	7027.330520	25.842701
177.912963	7021.325185	25.847719
178.037887	7035.301512	25.852736
177.896465	7053.917237	25.857754
178.080540	7064.596046	25.862772
178.133263	7073.239990	25.867789
178.385151	7083.296349	25.872807
178.530505	7099.987619	25.877824
178.808209	7120.075512	25.882842
179.327820	7129.952096	25.887860
179.450802	7153.095844	25.892877
179.553399	7148.565525	25.897895
179.939333	7153.069445	25.902912
180.249564	7176.854116	25.907930
179.991456	7183.016402	25.912948
180.475984	7178.558323	25.917965
181.162828	7195.157680	25.922983
181.049033	7197.919292	25.928000
181.325364	7203.339328	25.933018
181.666548	7205.282831	25.938036
181.198579	7210.911167	25.943053
181.569462	7222.588654	25.948071
181.584688	7236.506127	25.953088
181.848399	7231.688387	25.958106
182.178339	7250.669769	25.963124
181.851567	7260.333679	25.968141
182.410079	7262.986358	25.973159
182.622451	7285.052125	25.978176
182.478471	7291.103398	25.983194
182.678722	7302.014419	25.988212
182.670156	7321.024359	25.993229
183.376539	7333.885415	25.998247
183.712308	7348.027970	26.003264
183.786102	7355.706812	26.008282
183.981882	7355.203427	26.013300
184.150426	7368.520619	26.018317
184.389543	7378.791956	26.023335
184.546134	7388.040362	26.028352
184.704522	7384.832724	26.033370
185.166037	7393.401286	26.038388
185.205788	7410.213552	26.043405
185.266026	7408.592816	26.048423
185.615848	7415.172844	26.053440
185.503258	7426.795830	26.058458
185.868322	7431.347397	26.063476
185.874703	7438.561672	26.068493
186.155630	7456.019351	26.073511
186.236787	7468.341271	26.078528
186.236457	7475.192760	26.083546
186.470548	7482.869543	26.088564
186.951528	7500.412304	26.093581
187.228502	7496.733661	26.098599
186.931338	7499.183035	26.103616
187.124102	7514.105602	26.108634
187.499593	7526.960158	26.113652
187.612701	7527.734710	26.118669
187.776834	7543.272510	26.123687
187.874474	7557.589373	26.128704
188.159488	7563.116799	26.133722
188.292405	7569.303505	26.138740
188.561602	7582.359238	26.143757
188.587714	7583.935108	26.148775
189.423909	7606.959862	26.153792
189.214729	7619.075539	26.158810
189.672913	7615.953706	26.163828
189.569101	7636.934080	26.168845
189.797307	7643.003425	26.173863
190.287084	7640.529363	26.178880
190.204160	7643.263884	26.183898
190.681702	7662.999573	26.188916
190.573155	7670.247159	26.193933
190.706363	7669.294105	26.198951
191.075290	7683.488973	26.203968
191.066347	7694.133994	26.208986
191.470426	7709.325814	26.214004
191.329536	7717.545293	26.219021
191.789753	7717.096581	26.224039
191.866612	7723.807789	26.229056
192.013979	7748.957807	26.234074
192.622331	7756.256102	26.239092
192.447520	7766.876644	26.244109
192.734638	7778.163527	26.249127
192.852488	7787.078289	26.254144
193.005301	7798.392936	26.259162
193.434322	7805.643747	26.264180
193.456153	7824.557093	26.269197
193.651627	7815.918257	26.274215
194.181093	7828.808221	26.279232
194.173715	7846.976526	26.284250
194.562899	7846.607315	26.289268
194.506106	7861.452580	26.294285
194.458425	7873.819775	26.299303
194.732764	7882.133651	26.304320
194.929810	7889.785255	26.309338
195.199150	7898.971180	26.314356
194.974377	7915.391379	26.319373
195.372352	7928.516664	26.324391
195.839443	7935.544611	26.329408
195.812491	7944.751258	26.334426
196.287148	7956.435738	26.339444
196.421461	7973.602383	26.344461
196.252558	7989.629789	26.349479
196.469970	7996.907057	26.354496
196.395078	8007.735717	26.359514
197.207071	8019.775586	26.364532
197.258546	8042.927739	26.369549
197.448595	8047.461983	26.374567
197.804141	8058.335211	26.379584
197.870989	8074.155098	26.384602
198.539807	8086.101351	26.389620
198.466102	8093.852231	26.394637
198.759497	8091.495689	26.399655
198.818868	8101.886265	26.404672
198.811270	8115.760233	26.409690
199.207700	8116.717924	26.414708
199.217959	8137.049888	26.419725
199.337350	8145.232008	26.424743
199.769751	8153.928689	26.429760
199.646422	8174.149690	26.434778
200.321357	8177.797061	26.439796
200.300493	8182.565558	26.444813
200.651806	8207.681747	26.449831
201.079288	8211.388999	26.454848
201.129328	8214.695554	26.459866
201.508678	8202.919257	26.464884
201.619611	8217.855244	26.469901
201.680539	8237.540097	26.474919
202.179954	8233.920564	26.479936
202.067557	8243.320344	26.484954
202.464238	8237.365649	26.489972
202.512116	8247.618794	26.494989
202.872541	8258.936421	26.500007
202.853849	8265.521096	26.505024
202.840788	8261.179761	26.510042
203.153536	8282.656035	26.515060
203.161542	8297.304284	26.520077
203.271688	8303.380037	26.525095
203.449606	8319.602430	26.530112
203.428998	8348.400852	26.535130
203.769881	8356.614945	26.540148
203.790388	8368.441086	26.545165
204.467379	8382.562733	26.550183
204.438804	8395.662917	26.555200
204.582964	8423.138363	26.560218
205.407152	8430.168855	26.565236
205.265726	8429.606255	26.570253
205.666913	8449.394161	26.575271
205.914800	8445.148218	26.580288
205.618528	8464.547455	26.585306
205.986498	8475.615059	26.590324
206.327224	8490.298992	26.595341
206.506223	8509.996142	26.600359
206.888229	8519.430032	26.605376
206.977197	8543.235259	26.610394
207.243359	8548.807901	26.615412
207.556467	8548.843571	26.620429
207.292073	8573.084674	26.625447
207.837163	8571.305565	26.630464
207.947594	8598.500155	26.635482
208.532266	8603.463935	26.640500
208.621275	8607.258039	26.645517
208.616592	8633.951044	26.650535
209.048500	8637.368560	26.655552
209.196413	8640.969374	26.660570
209.623178	8662.075946	26.665588
209.469196	8663.295738	26.670605
209.906411	8671.921797	26.675623
210.467930	8672.555211	26.680640
210.595391	8692.781037	26.685658
211.036120	8687.948525	26.690676
211.203792	8687.308747	26.695693
211.196409	8691.281107	26.700711
211.509053	8716.131936	26.705728
211.548106	8725.554978	26.710746
211.660595	8709.737187	26.715764
211.742139	8724.844730	26.720781
211.786777	8737.297354	26.725799
211.995458	8746.185011	26.730816
212.065886	8759.461315	26.735834
212.566742	8773.176840	26.740852
212.544744	8781.737974	26.745869
212.533496	8805.132428	26.750887
212.784698	8810.082945	26.755904
212.851420	8844.776007	26.760922
213.343202	8848.942272	26.765940
213.773342	8862.558507	26.770957
213.847610	8873.370147	26.775975
214.110486	8879.470464	26.780992
214.289512	8914.939940	26.786010
214.386324	8907.076258	26.791028
214.505551	8918.396472	26.796045
214.639781	8924.224267	26.801063
215.118431	8931.696620	26.806080
215.018741	8958.698156	26.811098
215.310501	8951.680540	26.816116
215.743857	8970.965898	26.821133
215.593748	8980.193529	26.826151
216.303398	9000.927581	26.831168
216.540009	9017.621506	26.836186
216.714548	9021.908086	26.841204
217.089295	9030.566739	26.846221
217.239505	9046.179996	26.851239
217.412514	9056.138011	26.856256
217.467620	9074.439165	26.861274
217.600094	9084.047046	26.866292
218.153844	9082.127015	26.871309
218.375878	9106.706702	26.876327
218.485447	9107.767881	26.881344
218.637885	9129.583793	26.886362
218.604241	9137.752369	26.891380
219.108539	9153.785291	26.896397
219.179852	9180.091642	26.901415
219.800387	9169.720285	26.906432
219.696248	9202.981080	26.911450
219.973372	9201.234452	26.916468
220.542825	9210.966225	26.921485
220.550739	9224.480145	26.926503
220.919805	9222.286589	26.931520
221.093285	9240.155538	26.936538
221.385372	9260.110614	26.941556
221.771186	9250.581602	26.946573
221.564907	9264.465823	26.951591
222.023286	9270.920726	26.956608
222.303976	9289.472320	26.961626
222.311270	9290.358224	26.966644
222.483572	9305.865664	26.971661
222.649507	9320.165711	26.976679
222.806306	9328.358001	26.981696
223.104808	9356.155334	26.986714
223.180331	9363.956175	26.991732
223.663905	9380.285025	26.996749
223.934912	9383.027422	27.001767
224.261417	9391.064027	27.006784
224.005746	9413.223614	27.011802
224.358978	9417.954968	27.016820
224.512571	9435.475284	27.021837
224.536462	9446.010470	27.026855
225.140233	9461.549045	27.031872
225.399817	9479.526902	27.036890
225.128606	9496.977384	27.041908
225.502737	9502.768038	27.046925
225.637887	9523.175620	27.051943
225.744616	9533.813743	27.056960
226.392417	9548.088578	27.061978
226.781725	9564.245726	27.066996
227.385616	9591.587195	27.072013
227.553680	9594.847712	27.077031
227.898972	9592.148337	27.082048
227.781901	9604.773360	27.087066
227.833173	9624.421338	27.092084
228.148913	9621.168300	27.097101
228.250604	9641.836031	27.102119
229.099774	9645.989824	27.107136
229.183589	9641.550146	27.112154
229.168178	9644.596041	27.117172
229.925411	9656.691918	27.122189
229.623039	9675.216011	27.127207
229.937037	9680.512491	27.132224
229.989171	9673.476723	27.137242
230.214064	9692.312965	27.142260
230.690701	9693.805793	27.147277
230.476961	9714.350157	27.152295
230.720334	9726.895122	27.157312
231.223572	9735.651846	27.162330
231.102916	9743.490863	27.167348
231.375236	9751.765085	27.172365
231.794578	9774.150602	27.177383
231.689954	9782.599110	27.182400
232.022467	9803.742489	27.187418
232.220071	9815.407239	27.192436
232.345517	9829.617542	27.197453
232.317510	9848.874771	27.202471
232.646521	9863.834489	27.207488
233.192374	9873.795890	27.212506
233.082183	9889.879284	27.217524
233.902472	9906.383759	27.222541
233.660076	9927.083610	27.227559
233.864097	9936.530473	27.232576
234.175637	9958.492129	27.237594
234.612600	9976.857146	27.242612
235.093397	9985.475128	27.247629
235.214614	9998.274510	27.252647
235.596627	10013.706163	27.257664
235.922679	10017.038301	27.262682
236.040883	10044.778440	27.267700
236.355196	10049.296623	27.272717
236.107400	10050.239767	27.277735
236.689652	10060.935024	27.282752
236.755843	10088.631064	27.287770
236.887356	10104.827496	27.292788
237.373018	10103.211694	27.297805
237.665193	10131.219403	27.302823
238.182274	10129.091037	27.307840
238.512550	10155.081162	27.312858
238.291684	10164.698553	27.317876
238.744274	10167.065958	27.322893
238.793613	10182.305469	27.327911
239.126038	10199.774955	27.332928
239.585414	10208.306004	27.337946
239.375089	10234.513381	27.342964
239.659460	10234.285169	27.347981
239.872246	10252.651374	27.352999
240.095712	10264.572941	27.358016
240.618202	10277.566101	27.363034
240.826180	10297.631720	27.368052
240.973470	10309.083777	27.373069
241.263842	10333.449192	27.378087
241.233867	10345.790937	27.383104
241.949648	10352.615707	27.388122
241.754793	10374.055917	27.393140
242.032814	10376.432557	27.398157
242.361181	10403.093061	27.403175
242.538916	10412.316871	27.408192
243.001908	10418.734449	27.413210
242.743475	10443.121553	27.418228
243.377189	10443.723404	27.423245
243.733779	10468.011882	27.428263
244.180478	10485.872440	27.433280
244.592382	10487.493452	27.438298
244.552135	10503.425642	27.443316
244.995353	10506.290992	27.448333
245.192351	10518.577174	27.453351
244.894927	10515.995078	27.458368
245.448919	10537.471469	27.463386
245.594289	10548.486760	27.468404
246.028859	10545.302895	27.473421
245.837638	10564.104260	27.478439
245.884857	10579.687999	27.483456
246.224910	10595.678651	27.488474
246.473437	10605.399015	27.493492
246.870416	10617.192063	27.498509
247.199296	10632.715044	27.503527
247.144518	10651.826397	27.508544
247.741535	10666.389539	27.513562
247.741825	10690.981571	27.518580
248.336096	10698.375740	27.523597
248.228375	10716.288942	27.528615
248.665281	10735.596323	27.533632
249.317273	10741.903171	27.538650
249.081797	10750.967890	27.543668
249.598861	10750.354496	27.548685
249.978394	10779.651984	27.553703
250.103055	10788.527897	27.558720
250.687269	10791.059543	27.563738
250.347388	10823.258918	27.568756
250.807759	10814.045186	27.573773
251.214801	10833.754709	27.578791
251.424938	10851.368053	27.583808
251.858558	10841.025791	27.588826
251.770758	10866.108540	27.593844
252.300738	10870.683435	27.598861
252.106641	10881.539276	27.603879
252.535128	10905.477732	27.608896
252.991014	10905.783655	27.613914
253.069686	10925.914795	27.618932
253.608514	10929.701954	27.623949
253.937617	10948.578354	27.628967
253.705339	10967.954248	27.633984
254.217140	10970.228461	27.639002
254.358075	10985.103754	27.644020
254.468644	10996.816860	27.649037
254.614212	11012.016013	27.654055
254.778994	11026.836974	27.659072
255.028686	11046.626381	27.664090
255.223817	11066.391754	27.669108
255.729158	11079.579069	27.674125
256.018311	11091.784251	27.679143
256.092581	11120.504171	27.684160
256.746662	11139.653177	27.689178
256.878983	11150.979887	27.694196
257.574615	11151.398976	27.699213
257.890603	11167.170424	27.704231
257.837855	11181.765963	27.709248
258.368376	11181.878326	27.714266
258.177557	11202.284482	27.719284
258.662312	11205.010721	27.724301
258.846629	11222.488503	27.729319
258.578090	11243.153395	27.734336
259.131066	11252.989206	27.739354
259.168447	11270.393666	27.744372
259.748546	11285.116172	27.749389
260.085720	11312.217148	27.754407
260.245670	11319.681928	27.759424
260.765550	11338.642235	27.764442
260.706412	11342.323631	27.769460
261.077403	11360.976124	27.774477
261.223021	11363.656107	27.779495
261.468465	11392.611327	27.784512
261.769326	11395.713136	27.789530
261.485008	11419.685263	27.794548
262.032776	11432.637356	27.799565
262.099885	11447.786876	27.804583
262.559606	11467.865066	27.809600
263.053781	11469.108557	27.814618
263.316301	11498.059564	27.819636
263.413665	11501.852183	27.824653
263.908099	11524.739048	27.829671
264.130565	11539.982696	27.834688
264.350416	11548.171983	27.839706
264.619391	11564.632343	27.844724
264.875835	11586.827527	27.849741
265.103736	11595.593821	27.854759
265.199069	11608.373553	27.859776
265.476932	11625.097237	27.864794
265.887822	11651.006307	27.869812
265.922309	11662.261326	27.874829
266.750090	11669.420316	27.879847
266.656927	11688.411606	27.884864
267.225804	11705.807341	27.889882
267.235041	11721.314949	27.894900
267.361985	11736.970122	27.899917
267.724150	11747.784885	27.904935
267.928209	11765.061433	27.909952
268.557688	11778.293380	27.914970
268.250735	11791.841087	27.919988
268.728821	11812.219221	27.925005
269.133027	11823.840194	27.930023
269.327957	11847.289237	27.935040
270.018069	11858.546168	27.940058
269.679071	11873.544273	27.945076
270.343647	11894.756765	27.950093
271.062466	11890.942536	27.955111
271.208426	11914.352507	27.960128
271.527125	11930.847556	27.965146
271.736560	11928.171869	27.970164
271.692372	11940.807922	27.975181
272.362801	11956.516740	27.980199
272.361316	11962.565083	27.985216
272.683538	11976.919620	27.990234
272.723656	11997.846390	27.995252
272.975585	12006.467105	28.000269
273.196853	12023.863996	28.005287
273.358412	12040.085760	28.010304
273.614501	12058.209688	28.015322
273.724235	12085.740417	28.020340
273.916426	12104.406032	28.025357
274.564488	12118.095329	28.030375
274.384144	12145.436226	28.035392
275.053501	12157.197921	28.040410
275.103343	12184.467687	28.045428
275.288355	12202.838343	28.050445
275.832468	12226.348319	28.055463
276.272604	12250.773780	28.060480
276.605331	12266.466314	28.065498
277.004464	12280.215866	28.070516
277.172823	12294.602458	28.075533
277.949033	12302.709485	28.080551
277.882608	12314.388234	28.085568
278.165294	12329.906312	28.090586
278.349077	12347.268782	28.095604
278.604747	12358.377360	28.100621
279.160640	12366.449976	28.105639
279.182199	12378.139419	28.110656
279.539146	12394.026627	28.115674
279.926240	12409.581078	28.120692
279.788122	12423.868811	28.125709
280.263723	12432.257319	28.130727
280.427137	12458.133004	28.135744
280.878545	12459.911578	28.140762
281.366125	12472.666457	28.145780
281.209200	12490.539333	28.150797
281.908475	12489.746015	28.155815
281.515376	12515.787982	28.160832
282.056473	12522.663880	28.165850
282.206515	12541.660031	28.170868
282.423940	12554.521154	28.175885
282.594542	12571.107558	28.180903
282.557925	12596.696671	28.185920
282.907837	12609.682465	28.190938
283.587655	12643.968597	28.195956
283.083823	12659.273643	28.200973
283.925711	12687.182176	28.205991
283.921898	12717.356643	28.211008
284.235467	12735.755475	28.216026
284.881725	12755.752380	28.221044
284.994715	12794.647631	28.226061
285.580605	12807.279338	28.231079
285.763853	12832.332862	28.236096
285.919888	12844.331321	28.241114
286.576604	12876.915054	28.246132
286.527116	12887.355889	28.251149
286.837263	12895.140084	28.256167
287.244805	12934.826876	28.261184
287.474080	12943.795392	28.266202
288.259865	12954.712615	28.271220
288.342372	12981.997220	28.276237
289.240341	12984.215684	28.281255
289.260356	13007.986903	28.286272
289.336631	13012.459441	28.291290
289.609549	13031.472070	28.296308
289.748052	13050.877316	28.301325
290.160993	13057.806176	28.306343
290.426057	13087.282807	28.311360
290.872913	13104.780619	28.316378
291.791577	13099.615552	28.321396
291.737826	13112.522006	28.326413
292.190704	13127.768405	28.331431
292.039066	13143.363884	28.336448
292.347967	13159.437876	28.341466
292.656973	13168.169535	28.346484
292.955394	13187.509073	28.351501
293.355211	13195.971987	28.356519
293.206281	13214.648065	28.361536
293.540389	13231.494899	28.366554
293.910905	13247.629697	28.371572
294.318836	13267.274273	28.376589
294.608159	13286.511422	28.381607
294.570423	13306.130533	28.386624
295.317512	13325.750557	28.391642
295.414906	13344.376553	28.396660
295.574708	13364.733680	28.401677
296.101944	13379.427451	28.406695
295.888509	13392.202962	28.411712
296.257925	13414.482805	28.416730
296.803070	13441.166798	28.421748
296.904517	13458.605546	28.426765
297.352983	13472.094212	28.431783
297.822689	13494.601839	28.436800
298.174854	13513.006193	28.441818
298.379840	13526.224740	28.446836
298.635823	13545.529177	28.451853
299.186453	13563.275070	28.456871
299.340623	13588.339297	28.461888
299.705094	13594.489995	28.466906
299.965571	13610.980629	28.471924
300.187097	13633.315196	28.476941
300.506086	13640.355994	28.481959
300.461689	13659.845824	28.486976
300.941118	13673.383115	28.491994
301.427514	13685.948451	28.497012
301.802327	13707.096236	28.502029
302.053683	13715.056037	28.507047
302.006517	13726.924879	28.512064
302.346999	13746.916887	28.517082
302.811937	13766.450189	28.522100
302.891506	13790.214263	28.527117
303.542839	13802.635763	28.532135
303.521941	13824.684487	28.537152
303.655552	13841.621877	28.542170
304.319590	13858.271330	28.547188
304.507433	13885.179100	28.552205
304.919637	13891.843670	28.557223
305.338815	13911.257064	28.562240
305.285096	13934.170297	28.567258
305.526466	13947.846512	28.572276
305.676715	13971.036510	28.577293
305.990742	13988.325586	28.582311
306.351248	14024.141066	28.587328
306.706372	14046.714128	28.592346
307.276485	14067.878909	28.597364
307.342529	14103.836292	28.602381
307.661654	14118.997014	28.607399
308.119274	14139.102500	28.612416
308.208936	14165.464337	28.617434
309.013168	14183.235122	28.622452
308.866431	14205.916693	28.627469
309.483509	14221.727955	28.632487
309.929119	14254.128742	28.637504
310.071618	14271.820034	28.642522
310.636164	14283.392592	28.647540
310.887845	14310.203811	28.652557
311.118677	14325.008966	28.657575
311.424323	14347.827042	28.662592
311.560862	14371.196395	28.667610
311.946926	14394.976807	28.672628
311.996100	14413.221138	28.677645
312.960792	14435.109114	28.682663
313.034378	14448.944336	28.687680
312.975177	14471.857651	28.692698
313.251768	14485.684517	28.697716
313.664499	14518.732732	28.702733
314.092908	14546.552142	28.707751
314.676141	14563.847700	28.712768
314.851839	14579.153948	28.717786
315.262662	14588.748969	28.722804
315.587588	14616.063943	28.727821
316.015361	14627.925745	28.732839
316.206955	14653.325842	28.737856
316.636225	14676.177499	28.742874
316.967072	14689.574741	28.747892
317.374075	14703.687542	28.752909
317.718387	14727.508447	28.757927
317.831183	14745.499898	28.762944
317.840143	14769.420504	28.767962
318.543646	14789.284348	28.772980
318.734330	14805.846057	28.777997
319.227673	14819.783905	28.783015
319.280340	14843.281292	28.788032
319.581063	14863.200865	28.793050
320.018618	14879.263136	28.798068
319.731511	14905.242488	28.803085
320.260312	14927.266322	28.808103
321.050442	14949.245354	28.813120
321.230301	14965.763308	28.818138
321.851063	14986.285721	28.823156
321.765152	15003.829628	28.828173
322.237962	15011.520140	28.833191
322.573651	15021.432044	28.838208
322.355135	15037.864705	28.843226
323.068430	15057.134631	28.848244
323.367614	15091.377011	28.853261
323.148018	15107.846170	28.858279
323.869014	15127.431708	28.863296
324.035191	15153.985788	28.868314
324.064221	15175.288852	28.873332
324.540546	15208.007973	28.878349
324.828251	15228.344669	28.883367
325.154995	15256.289289	28.888384
325.050154	15283.347097	28.893402
326.116267	15306.281780	28.898420
326.192668	15339.819186	28.903437
326.927643	15352.778104	28.908455
327.424439	15377.334419	28.913472
327.534526	15406.467328	28.918490
328.177007	15425.580761	28.923508
328.142708	15448.130372	28.928525
328.591561	15467.392541	28.933543
329.369778	15486.880772	28.938560
329.232145	15498.297744	28.943578
329.860129	15515.430861	28.948596
329.594641	15541.529000	28.953613
330.158821	15557.271504	28.958631
330.856658	15582.767349	28.963648
330.758682	15605.168520	28.968666
331.369027	15621.404669	28.973684
331.736210	15651.505788	28.978701
331.889807	15676.050005	28.983719
332.326779	15685.220502	28.988736
332.521210	15714.338418	28.993754
333.264546	15740.547296	28.998772
333.270293	15761.832905	29.003789
333.478279	15788.463050	29.008807
333.978662	15805.378009	29.013824
334.192418	15829.176412	29.018842
334.640651	15858.028751	29.023860
334.714151	15883.510190	29.028877
334.795300	15905.547963	29.033895
335.418948	15918.580926	29.038912
335.509606	15963.746518	29.043930
336.409591	15986.777432	29.048948
336.776627	16012.327123	29.053965
337.026384	16026.943111	29.058983
337.239450	16045.084887	29.064000
337.418688	16071.357716	29.069018
338.068827	16090.108125	29.074036
338.633082	16110.893495	29.079053
338.413547	16132.672401	29.084071
338.729855	16154.110444	29.089088
339.108668	16191.213823	29.094106
339.288666	16216.657657	29.099124
339.632986	16234.948150	29.104141
339.868360	16282.704065	29.109159
340.679408	16303.801908	29.114176
340.786692	16332.407296	29.119194
341.320067	16354.473271	29.124212
341.436685	16379.478615	29.129229
341.978388	16408.256547	29.134247
342.481718	16435.920162	29.139264
342.491543	16448.155104	29.144282
343.280740	16470.275041	29.149300
343.761694	16498.784189	29.154317
343.857530	16514.070778	29.159335
344.168051	16542.855686	29.164352
344.127287	16560.343332	29.169370
344.779316	16575.471712	29.174388
345.054555	16600.057066	29.179405
345.159969	16618.242511	29.184423
345.922508	16635.568900	29.189440
345.725906	16664.756368	29.194458
346.128072	16690.780483	29.199476
346.794428	16710.249277	29.204493
346.704777	16738.074600	29.209511
347.339212	16759.750809	29.214528
347.597831	16797.066174	29.219546
347.926914	16819.302147	29.224564
348.129814	16836.097166	29.229581
348.335745	16873.058874	29.234599
348.817169	16902.158176	29.239616
349.233033	16937.948767	29.244634
349.507200	16962.093470	29.249652
349.768776	16983.910505	29.254669
350.379623	17025.851305	29.259687
350.724664	17054.746460	29.264704
351.212033	17077.563462	29.269722
351.387734	17107.144063	29.274740
351.628803	17133.042636	29.279757
351.974722	17155.020908	29.284775
352.633525	17172.713401	29.289792
352.786146	17214.903921	29.294810
353.036390	17240.321937	29.299828
353.618774	17273.653405	29.304845
353.820251	17306.992816	29.309863
354.314624	17328.636207	29.314880
354.590805	17365.557434	29.319898
354.847725	17395.720965	29.324916
355.603489	17417.472537	29.329933
355.619546	17451.894356	29.334951
356.100274	17468.662946	29.339968
356.328978	17502.765929	29.344986
356.826135	17532.183735	29.350004
357.601322	17552.634924	29.355021
357.608067	17586.152152	29.360039
358.251314	17608.758074	29.365056
358.465996	17627.211862	29.370074
358.988876	17663.990455	29.375092
359.533713	17676.610661	29.380109
359.901098	17695.482211	29.385127
360.259293	17712.306010	29.390144
360.433098	17736.309238	29.395162
360.478132	17771.076877	29.400180
361.168561	17787.068604	29.405197
360.983205	17815.165367	29.410215
361.631352	17843.308657	29.415232
362.199897	17863.789704	29.420250
362.404729	17898.293124	29.425268
362.815284	17915.184130	29.430285
362.805144	17953.678432	29.435303
363.185743	17968.036441	29.440320
363.673543	18004.156351	29.445338
364.364007	18029.382905	29.450356
364.770455	18056.018525	29.455373
364.930156	18084.946151	29.460391
365.360773	18108.352510	29.465408
365.847427	18135.036463	29.470426
366.176048	18157.551755	29.475444
366.686073	18192.919597	29.480461
366.745296	18221.049077	29.485479
367.152340	18234.970999	29.490496
367.471193	18268.616077	29.495514
367.602920	18289.611352	29.500532
368.141861	18304.816789	29.505549
368.564039	18337.508501	29.510567
369.353876	18358.852103	29.515584
369.764487	18377.762992	29.520602
369.410752	18394.341159	29.525620
370.124350	18410.271325	29.530637
370.151668	18446.807349	29.535655
370.694220	18471.570356	29.540672
370.901658	18490.961137	29.545690
371.122723	18523.092178	29.550708
371.515804	18549.240523	29.555725
371.855412	18587.716233	29.560743
372.383950	18615.511736	29.565760
372.706648	18640.311384	29.570778
372.756517	18678.305566	29.575796
373.689738	18703.532376	29.580813
373.403861	18747.322226	29.585831
374.059434	18770.041198	29.590848
374.279628	18798.387785	29.595866
374.484610	18834.445952	29.600884
375.020935	18867.709416	29.605901
375.302309	18908.481413	29.610919
375.636556	18947.584708	29.615936
376.016989	18980.930954	29.620954
376.558293	19023.913029	29.625972
377.149804	19042.906662	29.630989
377.210236	19092.537803	29.636007
377.993209	19118.274099	29.641024
378.426451	19153.253098	29.646042
379.116522	19186.040866	29.651060
379.830582	19204.052724	29.656077
380.198747	19236.991616	29.661095
380.726159	19249.759369	29.666112
380.677245	19276.708787	29.671130
381.286389	19314.860938	29.676148
381.554219	19321.851158	29.681165
382.115381	19349.792255	29.686183
382.550951	19374.711470	29.691200
382.862785	19397.311618	29.696218
382.922378	19422.494930	29.701236
383.351714	19443.923242	29.706253
383.750465	19472.389613	29.711271
383.823335	19502.700928	29.716288
384.221559	19529.892056	29.721306
384.573638	19561.018062	29.726324
385.363859	19592.762140	29.731341
385.401656	19630.202377	29.736359
385.857384	19661.819068	29.741376
386.125344	19686.998244	29.746394
386.091649	19715.810925	29.751412
386.988198	19750.705032	29.756429
387.327572	19788.308544	29.761447
387.761066	19822.147459	29.766464
388.189383	19853.127380	29.771482
388.418259	19880.971433	29.776500
389.281968	19908.924876	29.781517
389.259055	19943.608951	29.786535
389.712705	19968.964350	29.791552
390.088038	20001.782162	29.796570
390.371518	20035.091373	29.801588
390.775489	20057.915229	29.806605
391.291689	20093.952974	29.811623
391.771086	20125.204002	29.816640
392.069928	20158.887726	29.821658
392.226912	20198.526216	29.826676
393.059851	20217.050812	29.831693
393.301994	20252.446853	29.836711
393.442097	20269.892678	29.841728
394.437856	20302.323023	29.846746
394.652354	20328.160002	29.851764
395.067942	20350.014284	29.856781
395.295178	20380.519208	29.861799
395.761992	20395.541414	29.866816
396.375903	20418.250605	29.871834
396.390562	20451.449047	29.876852
396.568755	20477.654891	29.881869
397.032828	20503.706249	29.886887
397.340613	20535.520926	29.891904
397.751079	20560.192218	29.896922
398.134550	20597.646769	29.901940
398.192365	20624.897589	29.906957
398.702119	20657.317613	29.911975
399.289262	20699.031917	29.916992
399.799845	20730.042409	29.922010
400.184866	20768.670122	29.927028
400.762247	20792.587286	29.932045
401.155943	20832.456125	29.937063
401.409951	20858.842368	29.942080
402.118142	20887.493272	29.947098
402.291988	20920.134949	29.952116
402.942245	20945.173903	29.957133
403.001359	20982.282515	29.962151
403.076767	21012.599282	29.967168
403.662250	21055.735343	29.972186
403.881918	21099.004586	29.977204
404.582596	21128.349314	29.982221
404.890991	21172.844926	29.987239
405.096384	21208.504483	29.992256
405.707976	21241.492159	29.997274
406.089908	21280.350177	30.002292
406.454133	21321.749733	30.007309
406.738281	21353.934088	30.012327
407.570654	21393.722188	30.017344
407.696337	21432.077420	30.022362
408.188582	21458.317953	30.027380
408.867117	21504.304680	30.032397
409.387204	21540.934579	30.037415
409.756262	21583.174378	30.042432
410.342481	21607.334056	30.047450
410.665773	21633.271707	30.052468
411.176702	21660.138584	30.057485
411.733561	21692.518115	30.062503
411.846116	21717.213603	30.067520
412.351300	21745.760812	30.072538
412.456703	21781.293064	30.077556
413.413472	21813.854192	30.082573
413.745230	21844.070105	30.087591
414.103402	21871.019363	30.092608
414.588376	21907.986992	30.097626
415.008827	21936.772449	30.102644
415.269954	21972.861160	30.107661
415.667541	22000.658715	30.112679
416.196391	22026.602369	30.117696
416.284490	22054.001850	30.122714
416.825033	22092.755069	30.127732
417.327381	22126.580909	30.132749
417.630960	22151.565504	30.137767
417.985612	22192.809519	30.142784
418.636783	22219.117963	30.147802
418.804709	22247.816445	30.152820
419.315811	22276.857111	30.157837
419.841492	22315.291630	30.162855
420.299460	22351.335954	30.167872
420.515757	22375.941121	30.172890
420.803521	22402.046666	30.177908
421.317510	22443.501443	30.182925
421.964240	22472.404890	30.187943
421.935344	22505.445847	30.192960
422.621628	22530.673567	30.197978
422.946257	22562.771525	30.202996
423.261982	22596.217636	30.208013
423.678655	22625.170456	30.213031
424.103999	22667.994958	30.218048
424.306807	22687.955851	30.223066
424.794626	22727.692161	30.228084
425.083865	22761.002640	30.233101
425.706342	22796.471939	30.238119
425.958434	22825.341959	30.243136
426.588040	22863.438841	30.248154
427.216311	22894.772854	30.253172
427.674176	22933.882281	30.258189
428.184716	22960.462720	30.263207
428.688865	22995.448996	30.268224
429.310540	23021.128087	30.273242
429.176174	23052.885062	30.278260
429.670018	23083.994103	30.283277
430.113376	23121.922124	30.288295
430.604496	23169.948613	30.293312
431.338755	23189.661298	30.298330
431.477971	23233.594250	30.303348
431.710085	23271.174379	30.308365
432.099232	23312.621977	30.313383
432.667965	23342.145346	30.318400
433.262494	23375.737653	30.323418
433.122360	23426.457046	30.328436
433.908622	23461.206783	30.333453
434.427293	23501.707754	30.338471
434.209850	23545.864536	30.343488
435.070175	23588.747096	30.348506
435.294118	23641.272379	30.353524
435.876922	23676.023111	30.358541
436.623861	23715.717267	30.363559
436.651384	23762.680445	30.368576
437.181918	23800.243890	30.373594
437.706889	23846.718119	30.378612
438.220717	23883.227953	30.383629
438.731257	23926.960885	30.388647
439.138420	23968.626292	30.393664
439.716503	24006.876187	30.398682
440.469405	24035.644873	30.403700
441.151983	24067.885125	30.408717
441.607509	24108.363293	30.413735
441.611726	24142.535785	30.418752
442.506633	24172.397702	30.423770
442.975395	24202.576208	30.428788
443.169063	24241.697666	30.433805
443.824099	24260.387046	30.438823
443.918790	24306.113700	30.443840
444.689644	24332.804592	30.448858
444.706029	24365.641375	30.453876
445.231909	24406.461853	30.458893
445.871359	24430.878527	30.463911
446.119920	24475.378489	30.468928
446.641097	24510.544835	30.473946
446.730054	24544.984813	30.478964
447.087784	24583.266157	30.483981
447.821027	24624.771960	30.488999
448.286627	24664.240480	30.494016
448.934651	24699.818327	30.499034
449.375696	24746.289967	30.504052
449.340809	24780.735143	30.509069
450.193760	24815.254241	30.514087
450.317990	24854.751308	30.519104
450.965860	24885.781369	30.524122
451.258880	24926.543847	30.529140
451.513627	24957.689564	30.534157
451.831387	24993.575008	30.539175
452.565943	25034.882878	30.544192
452.886966	25063.750004	30.549210
453.525073	25113.104439	30.554228
453.888635	25138.737968	30.559245
454.206703	25173.365233	30.564263
454.792163	25211.868933	30.569280
455.466307	25244.194807	30.574298
455.665925	25286.153253	30.579316
456.103282	25319.701271	30.584333
456.743313	25361.523931	30.589351
457.321173	25400.369963	30.594368
457.977868	25430.059018	30.599386
457.954978	25467.903808	30.604404
458.462371	25503.714775	30.609421
458.815296	25539.409441	30.614439
459.254120	25582.893514	30.619456
459.787299	25627.913965	30.624474
460.637646	25669.980143	30.629492
460.542790	25709.931790	30.634509
461.254779	25739.139091	30.639527
461.693357	25785.885216	30.644544
462.298576	25823.264098	30.649562
463.035109	25872.039811	30.654580
463.182486	25904.775842	30.659597
463.621656	25936.886410	30.664615
464.027801	25989.625297	30.669632
464.881676	26015.989645	30.674650
465.007575	26057.933781	30.679668
465.537183	26103.918132	30.684685
466.277295	26139.461644	30.689703
466.763578	26177.406677	30.694720
467.026662	26226.170268	30.699738
467.312437	26263.252839	30.704756
467.831407	26293.877786	30.709773
468.494038	26340.853302	30.714791
468.711594	26377.079957	30.719808
469.498781	26411.493284	30.724826
469.973121	26453.323937	30.729844
470.123401	26497.337535	30.734861
470.654309	26534.664016	30.739879
470.901340	26585.222975	30.744896
471.732828	26641.726068	30.749914
472.171176	26669.522893	30.754932
472.382161	26716.675116	30.759949
473.348271	26754.485231	30.764967
473.788447	26803.019258	30.769984
474.088145	26836.129305	30.775002
474.649871	26880.334451	30.780020
475.248730	26929.823610	30.785037
475.363249	26958.970979	30.790055
476.179199	26998.929441	30.795072
476.689852	27033.247821	30.800090
477.169056	27062.786105	30.805108
477.795976	27105.741322	30.810125
478.449752	27138.061506	30.815143
479.257537	27162.280711	30.820160
479.417225	27194.771094	30.825178
480.214160	27224.566216	30.830196
480.533332	27262.717941	30.835213
481.267394	27290.268092	30.840231
481.612501	27334.049683	30.845248
481.942810	27352.294603	30.850266
481.961558	27378.048461	30.855284
482.064368	27422.387718	30.860301
482.967677	27455.686124	30.865319
483.404395	27488.238467	30.870336
483.702897	27520.630778	30.875354
484.262992	27544.818954	30.880372
484.172926	27589.966584	30.885389
484.853227	27625.141348	30.890407
485.492490	27671.502889	30.895424
485.621928	27708.592344	30.900442
486.291409	27755.214096	30.905460
486.238003	27802.687475	30.910477
486.556645	27856.689453	30.915495
487.154404	27911.112295	30.920512
487.352904	27955.951284	30.925530
487.999140	28015.423345	30.930548
488.607478	28069.172987	30.935565
489.429681	28114.947059	30.940583
489.918891	28165.353819	30.945600
490.372080	28207.031314	30.950618
491.105523	28248.697234	30.955636
491.254631	28300.756950	30.960653
491.785778	28344.544999	30.965671
492.381321	28416.904419	30.970688
492.771650	28451.677714	30.975706
493.536961	28505.986356	30.980724
493.931130	28555.570807	30.985741
494.562958	28591.670431	30.990759
495.442528	28645.695599	30.995776
495.950216	28678.686404	31.000794
496.380429	28723.867597	31.005812
496.886906	28760.455224	31.010829
497.763374	28805.931893	31.015847
498.391909	28849.282350	31.020864
498.332850	28886.291929	31.025882
498.856654	28926.694375	31.030900
499.288451	28972.046308	31.035917
500.011956	29011.245457	31.040935
500.230615	29067.135396	31.045952
501.008972	29108.288007	31.050970
501.584276	29156.528611	31.055988
501.782398	29201.011205	31.061005
502.492527	29239.550555	31.066023
503.022398	29290.285098	31.071040
503.479834	29330.383971	31.076058
503.533945	29369.874528	31.081076
504.218055	29412.034093	31.086093
504.965595	29467.291987	31.091111
505.218121	29505.456494	31.096128
505.612656	29560.766790	31.101146
506.285086	29608.165971	31.106164
506.748694	29659.871656	31.111181
507.367324	29709.971200	31.116199
507.870071	29758.499953	31.121216
508.351425	29811.944700	31.126234
509.253684	29857.132734	31.131252
509.481114	29906.789621	31.136269
510.294927	29937.940101	31.141287
510.648107	29976.943986	31.146304
510.869403	30023.428268	31.151322
511.206708	30069.379205	31.156340
511.817262	30118.310733	31.161357
512.772610	30168.952171	31.166375
513.009860	30209.654246	31.171392
513.562860	30264.735458	31.176410
514.117653	30300.952322	31.181428
514.324237	30347.190643	31.186445
514.739965	30400.165311	31.191463
515.456077	30446.357437	31.196480
516.070486	30500.984357	31.201498
516.744014	30536.396435	31.206516
517.059056	30585.718919	31.211533
517.549553	30631.431425	31.216551
518.093773	30668.338615	31.221568
518.135063	30711.115655	31.226586
519.167801	30746.730593	31.231604
519.353526	30803.638001	31.236621
519.953783	30844.234146	31.241639
520.390772	30894.761523	31.246656
520.783054	30936.436661	31.251674
521.336733	30986.212986	31.256692
521.851975	31044.981852	31.261709
522.336965	31084.988669	31.266727
523.059220	31140.953317	31.271744
523.122580	31190.268655	31.276762
523.852999	31234.668308	31.281780
524.642409	31297.147387	31.286797
524.606640	31345.072316	31.291815
525.535358	31410.434743	31.296832
526.013086	31459.543431	31.301850
526.598302	31513.373721	31.306868
526.960309	31567.525089	31.311885
527.429239	31632.689911	31.316903
528.156771	31672.698944	31.321920
528.507896	31746.380966	31.326938
529.172472	31795.276658	31.331956
529.648569	31847.034026	31.336973
530.123123	31904.329465	31.341991
530.748577	31958.621445	31.347008
530.860466	32018.687733	31.352026
531.699984	32078.857851	31.357044
532.291397	32143.000866	31.362061
532.684558	32201.620228	31.367079
533.703762	32257.084891	31.372096
534.152159	32318.850927	31.377114
534.715971	32367.739630	31.382132
535.208082	32419.726368	31.387149
535.732905	32479.880502	31.392167
536.321991	32525.824563	31.397184
536.839264	32587.829421	31.402202
537.463254	32638.785222	31.407220
537.750739	32688.989043	31.412237
538.566645	32753.968037	31.417255
538.915023	32807.383898	31.422272
539.585000	32861.276832	31.427290
540.457948	32915.483453	31.432308
540.880377	32977.445408	31.437325
541.743893	33024.364592	31.442343
542.282731	33070.034374	31.447360
542.432338	33123.503008	31.452378
542.879736	33181.065816	31.457396
543.366622	33237.331635	31.462413
544.183862	33289.137734	31.467431
544.829585	33335.835019	31.472448
545.274424	33387.210750	31.477466
545.611592	33445.960235	31.482484
546.555840	33497.417738	31.487501
546.730124	33544.689017	31.492519
547.362026	33605.946339	31.497536
547.648112	33657.980252	31.502554
548.603914	33701.064427	31.507572
549.191628	33754.759091	31.512589
549.672527	33822.684877	31.517607
550.343559	33862.894383	31.522624
550.573898	33914.001020	31.527642
551.032397	33971.892736	31.532660
551.365244	34020.098375	31.537677
552.077800	34082.966037	31.542695
552.925105	34136.628361	31.547712
552.959279	34188.610828	31.552730
553.909714	34235.077011	31.557748
554.195133	34293.740015	31.562765
554.488192	34351.221679	31.567783
555.191408	34395.636892	31.572800
555.647831	34451.577060	31.577818
556.287032	34503.589714	31.582836
556.583391	34571.911798	31.587853
556.933230	34629.416516	31.592871
557.767964	34675.136116	31.597888
558.239024	34747.456830	31.602906
558.692745	34808.624674	31.607924
559.538219	34861.917082	31.612941
560.140331	34926.327116	31.617959
560.910041	34987.746250	31.622976
561.382298	35048.031343	31.627994
561.896095	35103.276057	31.633012
562.784110	35152.756240	31.638029
562.750947	35215.763891	31.643047
563.441019	35273.113380	31.648064
563.662309	35351.237478	31.653082
564.242382	35407.800825	31.658100
565.186250	35477.436243	31.663117
565.598545	35547.181981	31.668135
566.433868	35601.996303	31.673152
567.175731	35672.707387	31.678170
567.651544	35722.036421	31.683188
568.158539	35790.018984	31.688205
568.653664	35852.477504	31.693223
569.549876	35906.550473	31.698240
570.115388	35978.810008	31.703258
570.820555	36029.812529	31.708276
570.979262	36094.173866	31.713293
571.677522	36158.206288	31.718311
572.581664	36209.886521	31.723328
572.920186	36270.519756	31.728346
573.590948	36326.963673	31.733364
574.315587	36391.513321	31.738381
574.737846	36440.603843	31.743399
575.001547	36499.283936	31.748416
575.519165	36571.844134	31.753434
576.133152	36633.872228	31.758452
576.693474	36684.761693	31.763469
577.594353	36762.703694	31.768487
578.419836	36818.287145	31.773504
578.975153	36875.973337	31.778522
579.499528	36933.516489	31.783540
580.228531	36972.621831	31.788557
580.690367	37052.787137	31.793575
581.213035	37098.529808	31.798592
581.908126	37163.595259	31.803610
582.645774	37212.812440	31.808628
583.175599	37281.472276	31.813645
583.503699	37340.018181	31.818663
584.471476	37394.399391	31.823680
584.644344	37458.125647	31.828698
585.171201	37509.379630	31.833716
585.827060	37563.689861	31.838733
586.100507	37634.669186	31.843751
586.951825	37691.488337	31.848768
587.571800	37758.749408	31.853786
587.753711	37812.939951	31.858804
588.651732	37886.190527	31.863821
588.999432	37952.010692	31.868839
590.174016	38018.151960	31.873856
590.497552	38080.277243	31.878874
590.750344	38135.214563	31.883892
591.671480	38196.824711	31.888909
592.014222	38260.090070	31.893927
592.737333	38305.490121	31.898944
593.078892	38368.790773	31.903962
593.819273	38428.985939	31.908980
594.232295	38486.713410	31.913997
594.668344	38549.067880	31.919015
595.821059	38607.295178	31.924032
596.191332	38670.614221	31.929050
597.014173	38730.029694	31.934068
598.007589	38782.324326	31.939085
598.087116	38844.006469	31.944103
598.604863	38897.614358	31.949120
599.160688	38949.202194	31.954138
599.563029	39017.217304	31.959156
600.271555	39071.810565	31.964173
600.881023	39146.916375	31.969191
601.429577	39197.533872	31.974208
602.004776	39274.495665	31.979226
602.527713	39331.298498	31.984244
603.232895	39404.738593	31.989261
603.804883	39471.057435	31.994279
604.323986	39535.598577	31.999296
605.105161	39602.536720	32.004314
605.597316	39670.318421	32.009332
606.265110	39732.755374	32.014349
606.432337	39812.110278	32.019367
607.426466	39880.693589	32.024384
608.087443	39947.551861	32.029402
608.704293	40022.559015	32.034420
609.388277	40096.002224	32.039437
609.835672	40161.870655	32.044455
610.853554	40223.455836	32.049472
611.531246	40287.408307	32.054490
611.982219	40358.103637	32.059508
612.929081	40419.322404	32.064525
613.631727	40488.038287	32.069543
614.340580	40547.033390	32.074560
615.166395	40611.047712	32.079578
616.062742	40666.277584	32.084596
616.658445	40715.777079	32.089613
616.798624	40771.978429	32.094631
617.499622	40824.336739	32.099648
618.077003	40883.686148	32.104666
618.383360	40953.375371	32.109684
619.157797	41012.070672	32.114701
620.035318	41083.058097	32.119719
620.762518	41133.979689	32.124736
621.133132	41205.035668	32.129754
621.698694	41262.632967	32.134772
622.298054	41323.744913	32.139789
622.691800	41386.958924	32.144807
623.382359	41447.175381	32.149824
623.762789	41511.528549	32.154842
624.506815	41583.221901	32.159860
625.277702	41658.222843	32.164877
625.588296	41729.514915	32.169895
626.315353	41794.291589	32.174912
626.839659	41853.627633	32.179930
627.355030	41932.422588	32.184948
628.380759	41989.810256	32.189965
628.832019	42067.669257	32.194983
629.713466	42125.911543	32.200000
630.196687	42187.831680	32.205018
630.575602	42261.068764	32.210036
631.609986	42321.534261	32.215053
632.015749	42404.501035	32.220071
632.645726	42472.405967	32.225088
633.541203	42522.384788	32.230106
634.232147	42588.332060	32.235124
634.908130	42643.989474	32.240141
635.591275	42697.120081	32.245159
635.582085	42749.093016	32.250176
636.445366	42805.474506	32.255194
636.743946	42871.165656	32.260212
638.066555	42932.785216	32.265229
638.106292	42998.314416	32.270247
638.718347	43063.490257	32.275264
639.502836	43131.750904	32.280282
639.838365	43198.112755	32.285300
640.791512	43262.544561	32.290317
641.264068	43336.357639	32.295335
642.103633	43401.999038	32.300352
642.678726	43464.795434	32.305370
643.266204	43537.633611	32.310388
643.987863	43601.593392	32.315405
644.423081	43679.828034	32.320423
644.957112	43751.725509	32.325440
645.834191	43828.886768	32.330458
646.197490	43902.483348	32.335476
647.025898	43967.465515	32.340493
647.246729	44043.937399	32.345511
648.411859	44120.420709	32.350528
648.955558	44188.573493	32.355546
649.431838	44268.464635	32.360564
650.364189	44342.091934	32.365581
650.913975	44426.477361	32.370599
651.841163	44497.216984	32.375616
652.597858	44564.003408	32.380634
653.176334	44651.179530	32.385652
654.067363	44714.155185	32.390669
654.532743	44778.742376	32.395687
655.008188	44859.766585	32.400704
655.941415	44919.313107	32.405722
656.635404	44999.202911	32.410740
657.476724	45065.190867	32.415757
657.712714	45134.563155	32.420775
658.771282	45215.148234	32.425792
659.111369	45282.195594	32.430810
659.585534	45356.859445	32.435828
660.578082	45423.549903	32.440845
661.122752	45496.699579	32.445863
661.929090	45570.276748	32.450880
662.655012	45639.273008	32.455898
663.000309	45714.442725	32.460916
663.544455	45785.518969	32.465933
664.748994	45866.171097	32.470951
665.324507	45942.064653	32.475968
666.070778	46009.060021	32.480986
666.827074	46089.360958	32.486004
667.561922	46152.869350	32.491021
668.149413	46220.873818	32.496039
668.752802	46295.040003	32.501056
669.677717	46359.142893	32.506074
670.068874	46438.315210	32.511092
670.848534	46488.045870	32.516109
671.720414	46562.743416	32.521127
672.004398	46631.295356	32.526144
673.126458	46694.252028	32.531162
673.746353	46766.326790	32.536180
674.381395	46829.380273	32.541197
675.323394	46905.419161	32.546215
675.497809	46971.464102	32.551232
676.527122	47038.779446	32.556250
676.743311	47108.433820	32.561268
677.691130	47167.514473	32.566285
678.258485	47238.396525	32.571303
678.741388	47305.196876	32.576320
679.483946	47358.709777	32.581338
679.965400	47418.907354	32.586356
680.571122	47478.727704	32.591373
681.207291	47550.199559	32.596391
681.614470	47624.829729	32.601408
682.411937	47695.684886	32.606426
683.035525	47774.385333	32.611444
683.977736	47844.102291	32.616461
684.331091	47911.782043	32.621479
684.876720	47985.850682	32.626496
685.692284	48063.083613	32.631514
686.666630	48138.875739	32.636532
687.147722	48201.577095	32.641549
687.963475	48271.818683	32.646567
688.547479	48360.912151	32.651584
689.442090	48429.969588	32.656602
689.967110	48517.364959	32.661620
690.925451	48585.114389	32.666637
691.558028	48656.812051	32.671655
691.793344	48738.018850	32.676672
692.964312	48809.839616	32.681690
693.248636	48886.424724	32.686708
694.007277	48966.096265	32.691725
694.693996	49048.300355	32.696743
695.694956	49121.309508	32.701760
696.527205	49196.399758	32.706778
696.828318	49284.214660	32.711796
698.008420	49347.214703	32.716813
698.712975	49434.436103	32.721831
699.138979	49517.594938	32.726848
700.059387	49582.075774	32.731866
700.652421	49669.724120	32.736884
701.247362	49747.123508	32.741901
702.134548	49820.978485	32.746919
702.574878	49903.896576	32.751936
703.611932	49988.087071	32.756954
704.065665	50072.153342	32.761972
705.023465	50142.135068	32.766989
705.972078	50227.964697	32.772007
706.279728	50302.384848	32.777024
707.410223	50377.743054	32.782042
708.092108	50457.597705	32.787060
708.292135	50531.164787	32.792077
709.303264	50616.114041	32.797095
709.844108	50699.650626	32.802112
710.675396	50773.910157	32.807130
711.324047	50861.238848	32.812148
712.356942	50933.090377	32.817165
712.951106	51018.780001	32.822183
713.134482	51090.052484	32.827200
714.395914	51173.130769	32.832218
714.932948	51255.103689	32.837236
715.601330	51338.659831	32.842253
716.221744	51406.689872	32.847271
716.972299	51498.944750	32.852288
717.802949	51577.111608	32.857306
718.545462	51657.870878	32.862324
718.820006	51738.947963	32.867341
719.760461	51828.942924	32.872359
720.275189	51929.533731	32.877376
721.036990	51997.416096	32.882394
721.675707	52090.898932	32.887412
722.801103	52163.586266	32.892429
723.714619	52250.567816	32.897447
724.018471	52329.999924	32.902464
725.072138	52405.246042	32.907482
725.906615	52491.609974	32.912500
726.667489	52555.015177	32.917517
727.598504	52624.002605	32.922535
728.196248	52701.959793	32.927552
728.575981	52766.660702	32.932570
729.350784	52839.080025	32.937588
729.837363	52915.129517	32.942605
730.622120	52983.043101	32.947623
731.206113	53069.204623	32.952640
731.722472	53140.808582	32.957658
732.462350	53226.142630	32.962676
733.158382	53315.635213	32.967693
734.306624	53382.169594	32.972711
734.579988	53483.174759	32.977728
735.640222	53549.698995	32.982746
735.923638	53637.719698	32.987764
736.870765	53739.379209	32.992781
737.824450	53823.265225	32.997799
738.320515	53915.245057	33.002816
739.231510	53993.376691	33.007834
740.006995	54081.817117	33.012852
740.671445	54168.936838	33.017869
741.240251	54256.072767	33.022887
741.754152	54349.226872	33.027904
742.483761	54440.747195	33.032922
743.247382	54537.582380	33.037940
744.030798	54631.969546	33.042957
745.000730	54720.608131	33.047975
745.736532	54817.822080	33.052992
746.849676	54912.535148	33.058010
747.557638	55003.107565	33.063028
748.037283	55093.275867	33.068045
749.026195	55180.896090	33.073063
749.802620	55283.520625	33.078080
750.622767	55366.019922	33.083098
751.278006	55462.043501	33.088116
751.972049	55550.838861	33.093133
752.955608	55635.239447	33.098151
753.764085	55743.933350	33.103168
754.478418	55827.463070	33.108186
755.655831	55921.292019	33.113204
755.973327	56000.654511	33.118221
757.111480	56090.415106	33.123239
757.450385	56185.224417	33.128256
758.222179	56264.986729	33.133274
758.990863	56362.436604	33.138292
759.938568	56449.987099	33.143309
760.914210	56535.890416	33.148327
761.251694	56624.698999	33.153344
762.241744	56713.766534	33.158362
762.973056	56801.095284	33.163380
763.462151	56905.368124	33.168397
764.721009	56987.675191	33.173415
765.091859	57078.628781	33.178432
765.831727	57170.311641	33.183450
766.732458	57256.394750	33.188468
767.415891	57355.607680	33.193485
768.449599	57440.241430	33.198503
769.180064	57527.137459	33.203520
769.889711	57619.958535	33.208538
770.743356	57704.875962	33.213556
771.567718	57801.337818	33.218573
772.405099	57879.041916	33.223591
773.239109	57966.504108	33.228608
774.067565	58057.904637	33.233626
774.734940	58149.148962	33.238644
775.450914	58235.146763	33.243661
776.295402	58307.719879	33.248679
777.085694	58388.745189	33.253696
777.693275	58471.633736	33.258714
778.698684	58549.761325	33.263732
779.350274	58639.329460	33.268749
779.868309	58707.363621	33.273767
780.453733	58798.055670	33.278784
781.266558	58882.289653	33.283802
782.165844	58959.008122	33.288820
782.620789	59052.339279	33.293837
783.405607	59124.893610	33.298855
783.751632	59228.070913	33.303872
784.409668	59318.955524	33.308890
785.340748	59418.959242	33.313908
785.787361	59520.926936	33.318925
786.928345	59615.859914	33.323943
787.749901	59717.987777	33.328960
788.324583	59815.233685	33.333978
789.542740	59917.069426	33.338996
790.322159	60023.162156	33.344013
791.457321	60109.187074	33.349031
791.963709	60207.425776	33.354048
793.051133	60313.424833	33.359066
793.749985	60406.917804	33.364084
794.416688	60500.113150	33.369101
795.399503	60601.106416	33.374119
796.103337	60691.711505	33.379136
796.771382	60791.860300	33.384154
797.646130	60889.396687	33.389172
798.594721	60994.543724	33.394189
799.742369	61074.875984	33.399207
800.227797	61187.937956	33.404224
800.884641	61282.661740	33.409242
802.022554	61385.617869	33.414260
802.555976	61486.519198	33.419277
803.590861	61578.533510	33.424295
804.336045	61686.473526	33.429312
805.141914	61781.920803	33.434330
806.243407	61876.194546	33.439348
806.713470	61979.093471	33.444365
807.409800	62074.421173	33.449383
808.269984	62174.734578	33.454400
809.325074	62278.322009	33.459418
810.100215	62372.310691	33.464436
810.750787	62472.919378	33.469453
811.956567	62570.390055	33.474471
812.507547	62679.663195	33.479488
813.290322	62773.804151	33.484506
814.277542	62873.271908	33.489524
815.196034	62977.087724	33.494541
816.036067	63073.078953	33.499559
816.606065	63167.497102	33.504576
817.460419	63276.723226	33.509594
818.512414	63369.077745	33.514612
818.509086	63461.708374	33.519629
819.425961	63572.177307	33.524647
820.195700	63684.042872	33.529664
821.199451	63779.997663	33.534682
822.112421	63881.669712	33.539700
822.930827	63996.550490	33.544717
823.688611	64095.158130	33.549735
824.841696	64195.888051	33.554752
825.481370	64300.932407	33.559770
826.510795	64402.575105	33.564788
827.082849	64512.202117	33.569805
828.275720	64608.919647	33.574823
829.213443	64722.172720	33.579840
830.017414	64811.243241	33.584858
831.274236	64906.099357	33.589876
831.456804	65003.200763	33.594893
832.416335	65086.165328	33.599911
833.148274	65182.670969	33.604928
833.820326	65275.558302	33.609946
834.641276	65364.893893	33.614964
835.611347	65455.950007	33.619981
836.525133	65544.822167	33.624999
836.936586	65641.989832	33.630016
837.854625	65738.688525	33.635034
839.100091	65830.819689	33.640052
839.583069	65935.942452	33.645069
840.505373	66031.168787	33.650087
841.095584	66128.909728	33.655104
841.682491	66235.666836	33.660122
842.736720	66331.454339	33.665140
843.410477	66447.617980	33.670157
844.516079	66549.138411	33.675175
845.330762	66659.431981	33.680192
846.240162	66763.849824	33.685210
847.090780	66860.084355	33.690228
847.620404	66965.229841	33.695245
848.562993	67076.098727	33.700263
849.556074	67187.219059	33.705280
850.112699	67295.687248	33.710298
851.161439	67409.973350	33.715316
852.042579	67526.658685	33.720333
852.761356	67623.063920	33.725351
853.583047	67733.703361	33.730368
854.383325	67859.489265	33.735386
855.597189	67970.381203	33.740404
856.263661	68084.373794	33.745421
857.254405	68198.951945	33.750439
858.335729	68308.166799	33.755456
859.066497	68429.231942	33.760474
860.240224	68536.099628	33.765492
861.110545	68644.902205	33.770509
861.977241	68744.304012	33.775527
862.965403	68859.967348	33.780544
863.794913	68966.053200	33.785562
864.776023	69065.658884	33.790580
865.339741	69179.813449	33.795597
866.336696	69283.628567	33.800615
867.593109	69399.579259	33.805632
868.024110	69500.276984	33.810650
869.148110	69610.484174	33.815668
869.912982	69722.901163	33.820685
870.760986	69831.631290	33.825703
871.671360	69934.161340	33.830720
872.138360	70043.309652	33.835738
873.456571	70159.121460	33.840756
873.945861	70267.514771	33.845773
875.211968	70382.172934	33.850791
876.005974	70486.710370	33.855808
876.671844	70600.153735	33.860826
877.661865	70705.292145	33.865844
878.401953	70817.187813	33.870861
879.280495	70933.405334	33.875879
880.496177	71043.762817	33.880896
881.095601	71168.172343	33.885914
882.162108	71258.586118	33.890932
883.216189	71370.723611	33.895949
883.837847	71486.461750	33.900967
884.800926	71596.433841	33.905984
885.324793	71713.555266	33.911002
886.739929	71828.677086	33.916020
887.313869	71932.922783	33.921037
888.372359	72034.907161	33.926055
889.464506	72145.044085	33.931072
890.278314	72263.284100	33.936090
891.426126	72361.859376	33.941108
892.220779	72454.808378	33.946125
892.779940	72553.753807	33.951143
893.771105	72645.937559	33.956160
894.440598	72749.526342	33.961178
895.111616	72845.520300	33.966196
895.821652	72962.212945	33.971213
896.343524	73072.322413	33.976231
897.392893	73185.336471	33.981248
898.129388	73319.493685	33.986266
899.248540	73413.980466	33.991284
899.988998	73537.178674	33.996301
900.827226	73657.932920	34.001319
901.785718	73778.705889	34.006336
902.540266	73906.058860	34.011354
903.229435	74018.681460	34.016372
904.414175	74151.846305	34.021389
905.230420	74275.814032	34.026407
906.124648	74405.847313	34.031424
907.035769	74542.348473	34.036442
908.477120	74658.442243	34.041460
909.227018	74788.564905	34.046477
909.914838	74908.408565	34.051495
910.992520	75031.559402	34.056512
911.620935	75152.305981	34.061530
912.775962	75279.619661	34.066548
913.878137	75411.932999	34.071565
914.397450	75538.202217	34.076583
915.448064	75660.178320	34.081600
916.493947	75797.107704	34.086618
917.689340	75924.867493	34.091636
918.423538	76045.190346	34.096653
919.323859	76174.126201	34.101671
920.194918	76305.009405	34.106688
921.186711	76432.337749	34.111706
922.212625	76553.981315	34.116724
923.206067	76687.085590	34.121741
924.035813	76815.840771	34.126759
924.978599	76951.497693	34.131776
925.959751	77073.916849	34.136794
927.010627	77197.381457	34.141812
928.227408	77320.193113	34.146829
929.005352	77453.660199	34.151847
929.855705	77583.782670	34.156864
930.779155	77716.493528	34.161882
931.762780	77840.592701	34.166900
932.633047	77963.730871	34.171917
933.389172	78099.754566	34.176935
934.584592	78219.500530	34.181952
935.051865	78353.397567	34.186970
936.087026	78490.750128	34.191988
937.181266	78619.554196	34.197005
938.251664	78748.426202	34.202023
939.359426	78877.526819	34.207040
940.237472	79011.789992	34.212058
941.205043	79144.596890	34.217076
942.461738	79271.309306	34.222093
942.860258	79392.388885	34.227111
943.873897	79524.197247	34.232128
944.655356	79653.267710	34.237146
945.616182	79782.631869	34.242164
946.726543	79922.865351	34.247181
947.679176	80052.238734	34.252199
948.691947	80174.909962	34.257216
949.638889	80301.622450	34.262234
950.361169	80436.476543	34.267252
951.535807	80568.352928	34.272269
952.040563	80698.050782	34.277287
953.349668	80829.178933	34.282304
954.020225	80940.302284	34.287322
954.710970	81068.219119	34.292340
956.097526	81183.438555	34.297357
956.624799	81317.602594	34.302375
957.627182	81443.198836	34.307392
958.519280	81574.052287	34.312410
959.340723	81703.905938	34.317428
960.443590	81828.070552	34.322445
961.532600	81967.232012	34.327463
962.763479	82095.394257	34.332480
963.347575	82228.719137	34.337498
964.295554	82362.338908	34.342516
965.295595	82499.177454	34.347533
966.022503	82638.681245	34.352551
967.257437	82772.781068	34.357568
968.137993	82913.273397	34.362586
969.025514	83055.486330	34.367604
969.625544	83206.396519	34.372621
970.615500	83342.855810	34.377639
971.498759	83493.714713	34.382656
972.326564	83642.419939	34.387674
973.520147	83796.279110	34.392692
974.649756	83933.237610	34.397709
975.707001	84091.581878	34.402727
976.833231	84236.090979	34.407744
977.723417	84391.022945	34.412762
978.749668	84544.889448	34.417780
979.793275	84685.859104	34.422797
980.427077	84842.994081	34.427815
981.588886	84996.588062	34.432832
982.645890	85144.790458	34.437850
983.460180	85301.481070	34.442868
984.589791	85448.812857	34.447885
985.810074	85604.299415	34.452903
986.920699	85752.844817	34.457920
987.849531	85905.521514	34.462938
989.007201	86044.626525	34.467956
989.890732	86199.090693	34.472973
990.997633	86344.103282	34.477991
991.988289	86502.329383	34.483008
993.129342	86641.725431	34.488026
994.312498	86793.593854	34.493044
995.475120	86934.652294	34.498061
996.233699	87086.940851	34.503079
997.151085	87221.688325	34.508096
998.279079	87376.277991	34.513114
998.998199	87521.501169	34.518132
1000.335856	87670.280585	34.523149
1000.932802	87826.549358	34.528167
1002.041283	87973.862486	34.533184
1003.045496	88125.452652	34.538202
1004.144058	88272.263016	34.543220
1005.182452	88424.608828	34.548237
1006.243406	88576.622813	34.553255
1007.033007	88720.886097	34.558272
1008.148811	88880.828720	34.563290
1009.100698	89024.358224	34.568308
1010.383762	89171.548645	34.573325
1011.224209	89325.091057	34.578343
1012.288542	89466.117513	34.583360
1013.120223	89619.005091	34.588378
1014.324139	89779.515061	34.593396
1015.291307	89922.806941	34.598413
1015.739644	90084.450153	34.603431
1016.819901	90229.946546	34.608448
1018.091511	90393.310026	34.613466
1018.565213	90541.718593	34.618484
1019.979258	90689.219443	34.623501
1020.818685	90841.423667	34.628519
1021.787379	90988.322795	34.633536
1022.723618	91127.627058	34.638554
1023.454330	91284.503863	34.643572
1024.488472	91429.704997	34.648589
1025.701151	91596.966092	34.653607
1026.396902	91747.813700	34.658624
1027.443767	91903.521972	34.663642
1028.547318	92065.342243	34.668660
1029.767165	92219.947969	34.673677
1030.456969	92387.054123	34.678695
1031.644658	92545.736991	34.683712
1033.066104	92702.179606	34.688730
1033.719150	92870.225571	34.693748
1034.929428	93028.167295	34.698765
1035.928049	93191.778321	34.703783
1036.986260	93343.151853	34.708800
1038.031342	93517.074572	34.713818
1039.098110	93692.077310	34.718836
1040.290313	93847.394166	34.723853
1040.907953	94011.390139	34.728871
1042.407308	94174.481836	34.733888
1043.473267	94341.134012	34.738906
1044.562951	94511.954776	34.743924
1045.505550	94673.122606	34.748941
1046.757493	94846.362200	34.753959
1047.619055	95003.285521	34.758976
1048.860099	95172.693224	34.763994
1049.778857	95346.605426	34.769012
1051.143191	95507.303826	34.774029
1051.801209	95681.020938	34.779047
1053.162368	95844.152828	34.784064
1054.228737	96015.595511	34.789082
1054.979942	96187.230754	34.794100
1056.138990	96348.538259	34.799117
1057.158924	96529.569958	34.804135
1058.022286	96707.121798	34.809152
1059.512090	96875.075607	34.814170
1060.061882	97052.884323	34.819188
1061.688323	97213.980854	34.824205
1062.701918	97394.488085	34.829223
1063.867475	97565.437531	34.834240
1064.895236	97731.884481	34.839258
1065.907125	97918.460553	34.844276
1067.100361	98069.169492	34.849293
1068.016661	98255.725878	34.854311
1069.408757	98429.885109	34.859328
1070.065203	98604.350772	34.864346
1071.491231	98784.723784	34.869364
1072.468013	98953.567649	34.874381
1073.431878	99123.060537	34.879399
1074.731847	99294.809827	34.884416
1075.608774	99467.934436	34.889434
1076.236438	99648.350619	34.894452
1077.896694	99810.540738	34.899469
1079.140732	99984.861736	34.904487
1080.518915	100161.725918	34.909504
1081.542422	100334.876490	34.914522
1082.334710	100497.113181	34.919540
1083.274966	100667.899171	34.924557
1084.271188	100840.221920	34.929575
1085.467288	101014.893422	34.934592
1086.855756	101178.909971	34.939610
1087.460289	101366.211797	34.944628
1088.536975	101532.111976	34.949645
1090.055215	101703.891986	34.954663
1091.127934	101873.182458	34.959680
1092.006323	102038.067609	34.964698
1092.720668	102202.233781	34.969716
1094.405781	102353.190578	34.974733
1094.777761	102524.310760	34.979751
1096.041452	102687.844635	34.984768
1097.437343	102844.132924	34.989786
1098.272104	103009.626663	34.994804
1099.148903	103182.763596	34.999821
1100.347430	103353.860214	35.004839
1101.252027	103526.779542	35.009856
1102.165192	103705.663492	35.014874
1103.004645	103888.803426	35.019892
1104.768657	104063.851139	35.024909
1105.595538	104244.880669	35.029927
1106.248172	104432.525883	35.034944
1107.471836	104609.996876	35.039962
1108.447260	104795.628273	35.044980
1109.621365	104989.321020	35.049997
1110.895692	105173.119897	35.055015
1111.975525	105364.361302	35.060032
1113.544446	105550.786438	35.065050
1114.488667	105752.223228	35.070068
1115.592496	105935.232342	35.075085
1116.716133	106109.829567	35.080103
1117.432998	106308.483763	35.085120
1118.856138	106509.809115	35.090138
1119.594653	106703.041769	35.095156
1121.028098	106897.452842	35.100173
1122.164593	107094.599604	35.105191
1123.149107	107287.314503	35.110208
1124.477006	107484.571816	35.115226
1125.126628	107697.864159	35.120244
1126.420802	107898.980623	35.125261
1127.573059	108108.583219	35.130279
1128.614929	108304.893192	35.135296
1130.014087	108510.860806	35.140314
1131.328916	108715.577263	35.145332
1132.571508	108919.255867	35.150349
1133.654789	109114.108187	35.155367
1134.622440	109314.035146	35.160384
1136.252666	109519.326209	35.165402
1137.190859	109713.434122	35.170420
1138.597564	109919.487187	35.175437
1139.712162	110113.505446	35.180455
1140.881250	110307.718754	35.185472
1142.263469	110494.183679	35.190490
1143.427218	110696.355835	35.195508
1144.596227	110888.888483	35.200525
1145.917460	111071.820461	35.205543
1147.045655	111271.887211	35.210560
1148.116953	111458.815464	35.215578
1149.164444	111659.113723	35.220596
1150.396683	111857.039282	35.225613
1151.909472	112048.864457	35.230631
1152.732452	112244.250791	35.235648
1153.922304	112436.296726	35.240666
1155.044834	112636.374286	35.245684
1156.083592	112826.864338	35.250701
1157.398543	113019.552390	35.255719
1158.091007	113216.816762	35.260736
1159.605044	113409.436587	35.265754
1160.722237	113617.668151	35.270772
1161.710769	113805.018612	35.275789
1163.084636	114007.243522	35.280807
1163.859016	114201.878781	35.285824
1165.189963	114404.227669	35.290842
1166.525003	114591.564099	35.295860
1167.530303	114793.462844	35.300877
1168.988866	114979.577831	35.305895
1170.062727	115173.866223	35.310912
1171.016739	115341.936739	35.315930
1171.790260	115536.175910	35.320948
1172.712529	115731.329392	35.325965
1174.087757	115917.920439	35.330983
1174.915096	116127.852874	35.336000
1175.954306	116316.592648	35.341018
1177.147293	116524.567030	35.346036
1178.206738	116723.049573	35.351053
1179.487009	116934.788272	35.356071
1180.431212	117145.912556	35.361088
1181.962982	117345.487015	35.366106
1182.959705	117559.101766	35.371124
1183.790081	117774.709576	35.376141
1185.390897	117989.735478	35.381159
1186.225803	118206.688882	35.386176
1187.307078	118422.855589	35.391194
1188.196749	118655.109981	35.396212
1189.547634	118873.909102	35.401229
1190.864964	119102.865197	35.406247
1191.941031	119340.542947	35.411264
1193.604550	119553.986144	35.416282
1194.581243	119791.493922	35.421300
1195.600888	120017.642606	35.426317
1197.210121	120251.260681	35.431335
1198.261042	120473.644161	35.436352
1199.634522	120706.278399	35.441370
1200.831989	120940.438889	35.446388
1202.181117	121170.749138	35.451405
1203.412161	121397.583127	35.456423
1204.255363	121621.403558	35.461440
1205.316422	121856.848428	35.466458
1206.685541	122095.311025	35.471476
1207.853279	122337.674021	35.476493
1209.333158	122565.641689	35.481511
1210.210128	122802.024237	35.486528
1211.325492	123037.393415	35.491546
1212.765437	123287.462363	35.496564
1214.078238	123526.173804	35.501581
1215.744017	123759.455277	35.506599
1216.271083	124001.265947	35.511616
1217.657364	124237.892431	35.516634
1218.868838	124487.033239	35.521652
1220.041813	124732.215565	35.526669
1221.830652	124976.753087	35.531687
1223.063056	125219.369396	35.536704
1224.397805	125449.220589	35.541722
1225.778891	125691.828755	35.546740
1226.712213	125919.836047	35.551757
1227.874122	126162.129294	35.556775
1229.178670	126402.233538	35.561792
1230.517544	126637.644392	35.566810
1231.696645	126878.026579	35.571828
1232.760048	127125.172744	35.576845
1234.313052	127359.007383	35.581863
1235.430710	127600.748885	35.586880
1236.920848	127836.726917	35.591898
1238.040986	128076.025421	35.596916
1239.375147	128311.475133	35.601933
1240.680408	128543.673834	35.606951
1242.000815	128782.171454	35.611968
1243.255674	129009.020227	35.616986
1244.840766	129240.341254	35.622004
1245.953260	129479.753168	35.627021
1247.203521	129704.706366	35.632039
1248.354525	129944.584451	35.637056
1249.419385	130155.666033	35.642074
1250.749964	130382.486829	35.647092
1251.838032	130600.995734	35.652109
1253.600571	130818.507312	35.657127
1254.491357	131034.871493	35.662144
1255.403796	131240.281122	35.667162
1256.783872	131474.111592	35.672180
1257.811910	131699.394541	35.677197
1259.142301	131915.856817	35.682215
1260.132125	132144.533889	35.687232
1261.284587	132370.155930	35.692250
1262.670703	132613.070349	35.697268
1263.778803	132856.463574	35.702285
1264.950601	133098.935345	35.707303
1265.993355	133334.140838	35.712320
1267.658791	133585.865117	35.717338
1268.848584	133815.256236	35.722356
1270.135400	134060.467178	35.727373
1271.231389	134306.877847	35.732391
1272.352935	134553.615768	35.737408
1273.535781	134803.071147	35.742426
1275.114204	135065.318449	35.747444
1276.067136	135313.839506	35.752461
1277.629474	135564.835361	35.757479
1278.561503	135830.758148	35.762496
1279.881374	136083.129227	35.767514
1281.472663	136333.618991	35.772532
1282.373883	136598.386605	35.777549
1283.618345	136859.600288	35.782567
1284.929947	137128.830541	35.787584
1286.035518	137383.554414	35.792602
1287.645505	137659.877784	35.797620
1288.824830	137934.144536	35.802637
1290.178076	138190.557929	35.807655
1291.664248	138462.077600	35.812672
1293.003329	138735.817285	35.817690
1294.427870	139001.151276	35.822708
1295.667574	139266.923634	35.827725
1297.512058	139537.162762	35.832743
1298.596912	139795.471179	35.837760
1300.107359	140063.601450	35.842778
1301.541717	140321.640506	35.847796
1302.333398	140593.355331	35.852813
1303.907405	140854.418499	35.857831
1304.966722	141127.475421	35.862848
1306.458718	141395.226015	35.867866
1307.856327	141650.072951	35.872884
1309.176825	141922.877394	35.877901
1310.993250	142188.488190	35.882919
1311.978870	142454.948445	35.887936
1313.119323	142717.885238	35.892954
1314.775096	142978.684523	35.897972
1316.013661	143244.005721	35.902989
1317.610437	143511.450851	35.908007
1318.729189	143774.437160	35.913024
1319.960136	144039.423195	35.918042
1321.435648	144300.249346	35.923060
1322.755047	144562.498170	35.928077
1324.318441	144823.909656	35.933095
1325.200215	145089.734787	35.938112
1326.669468	145358.800079	35.943130
1328.410752	145622.445335	35.948148
1329.353077	145885.996301	35.953165
1330.777243	146151.967904	35.958183
1332.078141	146407.308879	35.963200
1333.301273	146672.341009	35.968218
1334.941780	146934.122835	35.973236
1336.099155	147205.092335	35.978253
1337.076629	147469.105542	35.983271
1338.989596	147715.565577	35.988288
1339.879638	147968.930814	35.993306
1341.306723	148210.629712	35.998324
1342.258927	148459.511051	36.003341
1343.613238	148717.091481	36.008359
1344.846348	148981.060590	36.013376
1346.016462	149234.261379	36.018394
1347.611040	149486.658114	36.023412
1348.758006	149751.179615	36.028429
1349.915273	150015.739335	36.033447
1351.529944	150288.342712	36.038464
1352.716699	150553.180381	36.043482
1354.011769	150823.925252	36.048500
1355.368419	151100.432967	36.053517
1356.584603	151372.805634	36.058535
1358.035764	151652.536120	36.063552
1359.027674	151935.781922	36.068570
1360.800643	152209.349633	36.073588
1361.867053	152502.506261	36.078605
1363.419167	152777.395631	36.083623
1364.459124	153066.260970	36.088640
1365.826769	153360.097352	36.093658
1367.313679	153637.362933	36.098676
1368.246630	153942.374543	36.103693
1369.836743	154223.407271	36.108711
1371.528872	154523.820254	36.113728
1372.690394	154833.900354	36.118746
1374.189995	155115.918508	36.123764
1375.590341	155426.217511	36.128781
1376.858777	155707.339403	36.133799
1378.281280	156007.376978	36.138816
1379.498823	156317.662439	36.143834
1381.346646	156613.993590	36.148852
1382.474981	156910.344367	36.153869
1384.093350	157209.572112	36.158887
1385.231966	157521.808182	36.163904
1386.678713	157824.709685	36.168922
1388.309488	158128.039739	36.173940
1389.796838	158434.618027	36.178957
1391.030262	158737.916819	36.183975
1392.480914	159043.592353	36.188992
1393.882055	159344.127696	36.194010
1395.726362	159653.700865	36.199028
1396.872245	159963.074625	36.204045
1398.278190	160265.962913	36.209063
1399.788298	160560.767446	36.214080
1401.074338	160869.046436	36.219098
1402.859975	161169.544188	36.224116
1404.067854	161478.766742	36.229133
1405.726718	161781.040639	36.234151
1407.207377	162082.762549	36.239168
1408.491256	162381.639126	36.244186
1409.896108	162677.719288	36.249204
1411.115955	162993.383450	36.254221
1412.956315	163284.714193	36.259239
1414.320310	163591.756808	36.264256
1415.623695	163889.156281	36.269274
1417.228022	164189.210579	36.274292
1418.837581	164494.227067	36.279309
1420.152816	164786.720551	36.284327
1421.212889	165086.934455	36.289344
1422.903006	165392.286514	36.294362
1424.313240	165688.069270	36.299380
1425.721440	165992.380916	36.304397
1427.054610	166294.943375	36.309415
1428.548648	166587.990321	36.314432
1429.429405	166899.983112	36.319450
1431.287960	167185.969667	36.324468
1432.590460	167484.028137	36.329485
1434.101883	167769.758579	36.334503
1435.396122	168049.258407	36.339520
1436.467382	168355.380276	36.344538
1438.158799	168635.236837	36.349556
1439.371412	168932.494961	36.354573
1440.742528	169225.604830	36.359591
1442.216660	169522.658630	36.364608
1443.364297	169827.178931	36.369626
1445.132019	170120.317816	36.374644
1446.361378	170432.099698	36.379661
1447.760556	170735.543888	36.384679
1449.327838	171040.332776	36.389696
1450.736642	171356.697594	36.394714
1452.352934	171656.672966	36.399732
1453.473656	171981.135017	36.404749
1454.984062	172284.545506	36.409767
1456.483685	172599.533159	36.414784
1458.065241	172920.194598	36.419802
1459.431762	173233.571408	36.424820
1460.973026	173552.124470	36.429837
1462.094014	173870.139956	36.434855
1464.004871	174180.653786	36.439872
1465.125637	174508.292983	36.444890
1466.896921	174834.481676	36.449908
1468.465687	175159.538463	36.454925
1469.477336	175491.199922	36.459943
1471.506365	175816.870326	36.464960
1472.554232	176142.628873	36.469978
1474.332118	176468.725814	36.474996
1475.941171	176806.617598	36.480013
1477.366300	177136.216540	36.485031
1479.270361	177460.509641	36.490048
1480.064876	177792.869613	36.495066
1481.960067	178124.948358	36.500084
1483.583750	178456.249186	36.505101
1484.858702	178779.943973	36.510119
1486.493108	179109.203899	36.515136
1488.115179	179442.504009	36.520154
1489.594221	179767.377034	36.525172
1491.105641	180102.413109	36.530189
1492.586649	180432.519117	36.535207
1494.145730	180769.912355	36.540224
1495.540838	181103.577931	36.545242
1497.151412	181435.915392	36.550260
1498.804395	181773.401087	36.555277
1500.251201	182100.997407	36.560295
1501.983278	182427.127025	36.565312
1503.404554	182762.969149	36.570330
1504.611417	183092.819718	36.575348
1506.444575	183434.157413	36.580365
1508.103658	183764.737003	36.585383
1509.834692	184090.902225	36.590400
1511.009715	184422.466987	36.595418
1512.479243	184746.597648	36.600436
1513.957920	185088.867371	36.605453
1515.661810	185433.945301	36.610471
1517.452113	185757.813078	36.615488
1519.023371	186092.622633	36.620506
1520.183947	186422.767338	36.625524
1522.022481	186745.503106	36.630541
1523.631751	187070.220729	36.635559
1525.060691	187397.724549	36.640576
1526.842412	187733.727610	36.645594
1528.460179	188051.505851	36.650612
1529.792633	188362.262427	36.655629
1531.340576	188693.587527	36.660647
1532.695651	189013.013886	36.665664
1534.116004	189333.395959	36.670682
1535.527646	189641.696265	36.675700
1537.555014	189953.590493	36.680717
1539.120618	190250.583260	36.685735
1540.423449	190558.144636	36.690752
1541.691363	190876.630657	36.695770
1543.194344	191177.738698	36.700788
1544.624610	191491.631082	36.705805
1545.915796	191814.320125	36.710823
1547.683902	192121.482504	36.715840
1548.849047	192449.705262	36.720858
1550.132216	192783.153269	36.725876
1551.602961	193110.491173	36.730893
1553.225823	193445.943199	36.735911
1554.954475	193773.673597	36.740928
1556.286529	194120.907580	36.745946
1557.859665	194456.589025	36.750964
1559.371546	194802.108552	36.755981
1560.897057	195141.686244	36.760999
1562.581674	195489.567670	36.766016
1563.601366	195842.067747	36.771034
1565.234705	196188.069757	36.776052
1566.964619	196541.268784	36.781069
1568.639315	196895.964235	36.786087
1570.517661	197246.070143	36.791104
1571.926534	197607.224702	36.796122
1573.664276	197968.606184	36.801140
1575.428959	198310.585644	36.806157
1576.695830	198669.027022	36.811175
1578.746568	199023.239919	36.816192
1580.171768	199376.504215	36.821210
1581.832216	199738.237959	36.826228
1583.520042	200090.751521	36.831245
1584.975319	200451.837272	36.836263
1586.773393	200807.218313	36.841280
1588.468879	201168.979055	36.846298
1590.030446	201528.186356	36.851316
1591.486618	201871.542045	36.856333
1593.124545	202245.811259	36.861351
1594.805689	202599.036685	36.866368
1596.549718	202948.926859	36.871386
1598.415258	203316.155303	36.876404
1600.062828	203670.483369	36.881421
1601.634109	204030.285453	36.886439
1603.731397	204385.456803	36.891456
1604.919162	204744.652728	36.896474
1606.709210	205096.399161	36.901492
1608.289252	205445.655155	36.906509
1609.847503	205801.937960	36.911527
1611.515290	206155.982267	36.916544
1613.181660	206514.116995	36.921562
1614.548346	206868.277762	36.926580
1616.117753	207228.552245	36.931597
1617.947747	207596.378484	36.936615
1619.704708	207939.762757	36.941632
1621.252231	208304.121650	36.946650
1622.811134	208666.055019	36.951668
1624.676389	209023.190385	36.956685
1626.105047	209376.145636	36.961703
1628.030818	209737.489791	36.966720
1629.439675	210094.857548	36.971738
1630.839863	210448.647400	36.976756
1632.849173	210797.436625	36.981773
1634.294104	211164.402699	36.986791
1636.283918	211514.366293	36.991808
1637.629632	211874.520133	36.996826
1639.351659	212236.264069	37.001844
1641.147524	212573.514835	37.006861
1642.515419	212914.443936	37.011879
1644.569336	213232.403768	37.016896
1646.168658	213576.624150	37.021914
1647.432681	213891.567566	37.026932
1649.376145	214220.622251	37.031949
1650.884743	214558.842186	37.036967
1652.243441	214891.195925	37.041984
1653.696304	215227.268717	37.047002
1655.347561	215567.322749	37.052020
1657.189016	215920.451769	37.057037
1658.352723	216266.455698	37.062055
1660.401941	216627.400898	37.067072
1661.998216	216978.110702	37.072090
1663.215494	217327.589070	37.077108
1664.998186	217686.753540	37.082125
1666.560340	218046.006531	37.087143
1668.358215	218400.929549	37.092160
1670.177931	218779.089725	37.097178
1671.612247	219130.951339	37.102196
1673.186371	219487.591381	37.107213
1675.027266	219877.359214	37.112231
1676.850316	220232.157359	37.117248
1678.748184	220606.018848	37.122266
1680.359617	220978.201829	37.127284
1682.035532	221339.580856	37.132301
1683.286286	221722.417342	37.137319
1684.930899	222093.938250	37.142336
1687.033327	222472.166365	37.147354
1688.318927	222859.522051	37.152372
1690.461717	223236.425275	37.157389
1691.844157	223620.160806	37.162407
1693.315153	224020.468907	37.167424
1695.293233	224466.337842	37.172442
1696.557769	224858.046971	37.177460
1698.789005	225237.456540	37.182477
1700.179357	225640.501137	37.187495
1702.167983	226031.357802	37.192512
1703.702173	226425.516566	37.197530
1705.431468	226825.816567	37.202548
1707.656050	227197.816314	37.207565
1709.211360	227602.059096	37.212583
1710.841080	227998.391298	37.217600
1712.949194	228388.676538	37.222618
1714.353729	228776.564472	37.227636
1716.573348	229158.425917	37.232653
1718.014180	229556.444897	37.237671
1719.880406	229943.548605	37.242688
1721.828637	230325.407246	37.247706
1723.392338	230720.945298	37.252724
1725.128550	231110.943909	37.257741
1727.109956	231508.243939	37.262759
1728.764033	231892.517519	37.267776
1730.701323	232275.018003	37.272794
1732.261161	232670.841217	37.277812
1733.963422	233054.449280	37.282829
1735.676121	233444.102058	37.287847
1737.352785	233836.378069	37.292864
1739.034834	234224.894704	37.297882
1740.993723	234627.083334	37.302900
1742.669431	235006.001034	37.307917
1744.447707	235402.683768	37.312935
1746.178518	235780.425569	37.317952
1748.083159	236176.098489	37.322970
1749.943630	236568.705946	37.327988
1751.496892	236950.594591	37.333005
1753.249714	237349.800548	37.338023
1755.351352	237727.459656	37.343040
1756.877496	238107.043497	37.348058
1758.253087	238482.029754	37.353076
1759.980366	238858.330324	37.358093
1761.958724	239225.013495	37.363111
1763.653261	239596.850025	37.368128
1765.373363	239958.928516	37.373146
1766.914964	240332.239493	37.378164
1768.799624	240702.471550	37.383181
1770.090722	241082.886985	37.388199
1771.798630	241471.134339	37.393216
1773.902560	241854.211021	37.398234
1774.995185	242252.442808	37.403252
1776.730447	242632.431682	37.408269
1778.532401	243032.630539	37.413287
1780.216947	243439.428670	37.418304
1782.184810	243838.813854	37.423322
1783.691811	244239.672881	37.428340
1785.772861	244643.943229	37.433357
1786.952504	245050.649267	37.438375
1788.954082	245475.484686	37.443392
1790.805581	245890.260558	37.448410
1792.180136	246315.403891	37.453428
1794.199483	246732.667986	37.458445
1795.678984	247165.847761	37.463463
1797.517562	247588.832980	37.468480
1799.587053	248018.842563	37.473498
1801.474518	248457.367287	37.478516
1803.074726	248882.069886	37.483533
1805.092784	249313.511912	37.488551
1806.827063	249752.774568	37.493568
1808.965053	250189.735489	37.498586
1810.521812	250639.341939	37.503604
1812.488002	251068.075991	37.508621
1814.358283	251516.158019	37.513639
1816.088621	251952.603452	37.518656
1818.088259	252385.803912	37.523674
1819.539132	252853.872280	37.528692
1821.422508	253290.420332	37.533709
1823.329056	253738.040614	37.538727
1825.223205	254181.497047	37.543744
1827.392354	254628.896583	37.548762
1829.100878	255083.993370	37.553780
1830.966384	255527.683738	37.558797
1832.915719	255988.456818	37.563815
1834.500790	256438.951053	37.568832
1836.743982	256885.094348	37.573850
1838.654320	257341.860472	37.578868
1840.533402	257787.301947	37.583885
1842.345253	258234.532795	37.588903
1844.119626	258689.695680	37.593920
1846.079041	259136.825956	37.598938
1847.988663	259588.181375	37.603956
1849.748919	260037.275116	37.608973
1851.818085	260491.957296	37.613991
1853.749698	260944.172574	37.619008
1856.019807	261379.819696	37.624026
1857.511778	261837.238789	37.629044
1859.140529	262283.178252	37.634061
1861.346154	262731.003715	37.639079
1863.302575	263186.059246	37.644096
1864.923592	263624.353001	37.649114
1866.757639	264087.455675	37.654132
1868.608468	264527.870235	37.659149
1870.324252	264981.821305	37.664167
1872.011973	265434.506527	37.669184
1874.194387	265886.322208	37.674202
1875.948771	266335.591692	37.679220
1877.799893	266787.842380	37.684237
1879.615806	267235.627530	37.689255
1881.490459	267677.255016	37.694272
1883.334412	268096.659493	37.699290
1885.039196	268538.974642	37.704308
1887.016567	268972.632690	37.709325
1888.984394	269403.497512	37.714343
1890.674371	269839.970964	37.719360
1892.387654	270275.957386	37.724378
1894.116556	270722.863907	37.729396
1896.250657	271163.530034	37.734413
1897.983021	271612.924252	37.739431
1899.840756	272063.948299	37.744448
1901.644074	272513.558109	37.749466
1903.373018	272972.349870	37.754484
1905.215853	273431.223691	37.759501
1907.058208	273898.682894	37.764519
1908.950775	274364.735845	37.769536
1910.781722	274826.251088	37.774554
1912.756948	275301.814604	37.779572
1914.677192	275774.922241	37.784589
1916.794929	276249.926899	37.789607
1918.301852	276735.039946	37.794624
1920.528882	277202.683310	37.799642
1922.359632	277694.650186	37.804660
1924.100562	278174.717173	37.809677
1926.390731	278660.712639	37.814695
1928.199271	279150.037931	37.819712
1930.219120	279640.190786	37.824730
1932.318472	280126.874620	37.829748
1933.711098	280622.513733	37.834765
1935.971500	281114.731395	37.839783
1937.923949	281615.431921	37.844800
1940.149288	282116.314583	37.849818
1942.115865	282608.119388	37.854836
1944.044071	283100.030710	37.859853
1946.254846	283592.274937	37.864871
1947.985802	284095.138443	37.869888
1950.098011	284590.901279	37.874906
1952.096990	285096.867094	37.879924
1954.067919	285597.019041	37.884941
1956.213728	286080.934649	37.889959
1957.779169	286600.073908	37.894976
1960.075507	287088.889107	37.899994
1962.049042	287600.794361	37.905012
1963.647478	288104.936310	37.910029
1965.670008	288615.331114	37.915047
1967.774236	289120.732031	37.920064
1970.117411	289625.634374	37.925082
1972.011033	290138.838678	37.930100
1973.668865	290646.872859	37.935117
1976.296876	291149.385409	37.940135
1977.933658	291662.448180	37.945152
1980.095997	292171.815264	37.950170
1982.016873	292680.000899	37.955188
1983.801984	293194.734484	37.960205
1985.943576	293698.078798	37.965223
1988.055530	294204.143557	37.970240
1989.979215	294716.713973	37.975258
1991.775818	295228.922060	37.980276
1993.436940	295740.210399	37.985293
1996.070660	296238.382327	37.990311
1997.616387	296769.877009	37.995328
1999.863286	297281.416931	38.000346
2001.988449	297796.555663	38.005364
2003.783418	298301.434620	38.010381
2006.160278	298812.615377	38.015399
2007.941625	299322.241010	38.020416
2010.048363	299834.096142	38.025434
2012.020482	300341.577021	38.030452
2013.825030	300828.231383	38.035469
2015.865169	301312.380825	38.040487
2017.913141	301810.368149	38.045504
2020.703328	302287.048901	38.050522
2022.335613	302772.731243	38.055540
2024.091438	303252.955655	38.060557
2025.859413	303734.699353	38.065575
2027.498676	304229.998241	38.070592
2029.891637	304719.328702	38.075610
2031.409890	305234.222812	38.080628
2033.664153	305735.430699	38.085645
2035.682942	306239.899883	38.090663
2037.583426	306758.861396	38.095680
2039.563093	307259.420004	38.100698
2041.532033	307770.059516	38.105716
2043.754716	308288.450443	38.110733
2045.386844	308816.281129	38.115751
2047.639159	309340.476042	38.120768
2049.731115	309862.890959	38.125786
2051.699403	310396.775987	38.130804
2053.463945	310930.030771	38.135821
2055.779317	311465.831999	38.140839
2057.660479	312002.793157	38.145856
2059.761658	312547.789582	38.150874
2061.618210	313092.822467	38.155892
2063.999158	313640.380372	38.160909
2066.340018	314188.601084	38.165927
2068.067122	314739.966253	38.170944
2070.384962	315292.981841	38.175962
2072.326120	315840.011811	38.180980
2074.317382	316394.799538	38.185997
2076.524651	316946.627078	38.191015
2078.604249	317504.337008	38.196032
2080.788610	318057.556105	38.201050
2083.360275	318619.543242	38.206068
2085.422187	319184.428389	38.211085
2087.548961	319736.500687	38.216103
2089.541804	320299.889725	38.221120
2091.717970	320845.926870	38.226138
2093.839832	321404.460814	38.231156
2095.933570	321970.535664	38.236173
2098.174251	322526.678948	38.241191
2100.133203	323102.820714	38.246208
2102.519418	323657.203526	38.251226
2104.623176	324220.006732	38.256244
2106.472868	324775.890017	38.261261
2109.056721	325334.820761	38.266279
2111.030097	325912.279737	38.271296
2113.269329	326465.823695	38.276314
2115.507296	327027.233267	38.281332
2117.607109	327592.037025	38.286349
2119.815264	328150.597380	38.291367
2121.817615	328704.743488	38.296384
2123.873260	329269.512988	38.301402
2126.217664	329824.150446	38.306420
2128.789925	330387.224258	38.311437
2131.039554	330936.027475	38.316455
2132.940940	331505.471501	38.321472
2135.204436	332059.694208	38.326490
2137.248903	332620.547963	38.331508
2139.463825	333175.630632	38.336525
2141.579541	333723.438336	38.341543
2143.676505	334284.444052	38.346560
2146.087507	334838.258838	38.351578
2148.137346	335390.655181	38.356596
2149.945455	335947.375693	38.361613
2152.503882	336501.377248	38.366631
2154.644249	337055.670408	38.371648
2156.718761	337580.650147	38.376666
2158.940238	338091.867741	38.381684
2160.612421	338610.836695	38.386701
2162.703344	339145.494147	38.391719
2164.821412	339666.130140	38.396736
2166.910721	340199.939046	38.401754
2169.258992	340729.054535	38.406772
2171.237000	341269.165158	38.411789
2173.322412	341805.470253	38.416807
2175.067725	342353.247279	38.421824
2177.334064	342893.622347	38.426842
2179.577347	343443.462255	38.431860
2181.203993	344005.402684	38.436877
2183.689353	344558.768482	38.441895
2185.797928	345124.727736	38.446912
2187.953052	345683.540811	38.451930
2190.147864	346251.502619	38.456948
2191.936239	346832.036462	38.461965
2194.240366	347407.427497	38.466983
2196.009512	347997.872900	38.472000
2198.313502	348585.532286	38.477018
2200.501576	349173.812245	38.482036
2202.664772	349774.472801	38.487053
2204.824503	350374.618311	38.492071
2206.987282	350969.146945	38.497088
2208.861178	351576.784093	38.502106
2211.635619	352180.000986	38.507124
2213.732487	352783.422866	38.512141
2216.301832	353399.801255	38.517159
2218.196088	354017.753984	38.522176
2220.201817	354634.182266	38.527194
2223.044716	355249.397682	38.532212
2225.007062	355876.319938	38.537229
2227.103851	356484.459621	38.542247
2229.243395	357110.369899	38.547264
2231.687899	357738.732260	38.552282
2234.118273	358367.721647	38.557300
2236.293430	359000.041817	38.562317
2238.750909	359622.106174	38.567335
2241.028946	360262.863701	38.572352
2243.002975	360888.489465	38.577370
2245.495444	361519.220738	38.582388
2247.700684	362165.312793	38.587405
2249.931176	362790.333376	38.592423
2252.328106	363434.038880	38.597440
2254.471530	364067.932513	38.602458
2256.810298	364704.117372	38.607476
2258.726456	365344.724703	38.612493
2261.663770	365983.833617	38.617511
2263.832850	366616.742180	38.622528
2265.744499	367260.133620	38.627546
2268.295283	367905.133411	38.632564
2270.568276	368558.411719	38.637581
2272.894713	369198.505129	38.642599
2275.366136	369836.889397	38.647616
2277.441215	370485.904869	38.652634
2280.073397	371128.983116	38.657652
2282.189866	371774.240210	38.662669
2284.530707	372413.665933	38.667687
2287.038358	373062.386092	38.672704
2289.238331	373701.811958	38.677722
2291.785097	374340.382810	38.682740
2293.646105	374980.931968	38.687757
2295.932942	375616.631301	38.692775
2298.419708	376262.632972	38.697792
2300.115938	376908.372653	38.702810
2302.618075	377555.615546	38.707828
2304.936916	378191.236765	38.712845
2307.197826	378818.893160	38.717863
2309.260841	379434.474885	38.722880
2311.494148	380063.076291	38.727898
2313.868899	380674.526648	38.732916
2316.120608	381298.968579	38.737933
2318.425705	381928.435765	38.742951
2320.593318	382559.460307	38.747968
2322.679812	383195.404962	38.752986
2325.438813	383829.476772	38.758004
2327.498706	384463.068438	38.763021
2329.597670	385109.064429	38.768039
2332.199773	385751.440334	38.773056
2334.564940	386398.329818	38.778074
2336.754768	387044.601286	38.783092
2338.928590	387697.149346	38.788109
2341.164459	388348.000484	38.793127
2343.643240	389013.653311	38.798144
2345.745846	389685.083056	38.803162
2348.333538	390341.588895	38.808180
2350.161677	391011.894417	38.813197
2352.672071	391696.774624	38.818215
2354.987350	392377.742796	38.823232
2357.245515	393068.565107	38.828250
2359.591694	393751.195555	38.833268
2361.675866	394454.662670	38.838285
2364.242120	395135.375039	38.843303
2366.657898	395834.370164	38.848320
2368.979932	396537.900837	38.853338
2371.773561	397231.376904	38.858356
2374.167910	397940.640349	38.863373
2376.749803	398643.545375	38.868391
2379.139428	399346.110312	38.873408
2381.404644	400056.230286	38.878426
2384.062101	400755.903760	38.883444
2386.392215	401458.730903	38.888461
2389.030919	402161.971185	38.893479
2391.501526	402874.090185	38.898496
2393.776424	403581.586640	38.903514
2396.362441	404291.750294	38.908532
2398.737739	404997.623410	38.913549
2401.051389	405706.047656	38.918567
2404.091572	406414.409825	38.923584
2406.415327	407130.472319	38.928602
2409.023442	407827.012671	38.933620
2411.146608	408545.553823	38.938637
2413.814075	409247.114571	38.943655
2416.500413	409955.594882	38.948672
2419.104522	410664.804644	38.953690
2421.368926	411360.195778	38.958708
2423.922344	412081.306876	38.963725
2426.371830	412782.304044	38.968743
2428.914231	413480.607703	38.973760
2431.108680	414175.125649	38.978778
2433.772104	414887.606008	38.983796
2436.115077	415595.560914	38.988813
2438.550730	416290.666261	38.993831
2441.087706	417005.464377	38.998848
2443.525941	417709.090760	39.003866
2445.991352	418411.578988	39.008884
2448.016018	419115.690523	39.013901
2450.618044	419837.387451	39.018919
2453.150717	420536.716155	39.023936
2455.691686	421249.925113	39.028954
2458.228858	421957.467895	39.033972
2460.866735	422671.101183	39.038989
2463.025754	423372.032251	39.044007
2466.028500	424067.386075	39.049024
2468.233999	424768.421504	39.054042
2470.854638	425451.494806	39.059060
2472.906162	426114.035707	39.064077
2474.911102	426790.236331	39.069095
2477.880340	427455.171135	39.074112
2479.730707	428138.599270	39.079130
2482.411208	428816.605780	39.084148
2484.930416	429506.313856	39.089165
2486.948987	430188.035400	39.094183
2489.652761	430876.154383	39.099200
2491.940241	431574.648413	39.104218
2494.583199	432270.076453	39.109236
2496.796807	432976.538497	39.114253
2498.758527	433681.704609	39.119271
2501.682595	434393.827000	39.124288
2504.110504	435114.107216	39.129306
2506.271392	435830.916726	39.134324
2508.880676	436558.358904	39.139341
2511.025748	437293.749186	39.144359
2513.531640	438021.110936	39.149376
2515.848885	438774.693352	39.154394
2518.542655	439526.265466	39.159412
2520.842783	440273.373801	39.164429
2523.535151	441023.984896	39.169447
2526.132314	441791.991791	39.174464
2528.328920	442556.749355	39.179482
2530.961019	443320.700159	39.184500
2533.469093	444088.388587	39.189517
2535.903268	444867.242631	39.194535
2538.516473	445644.825077	39.199552
2540.837716	446432.039185	39.204570
2543.572987	447216.374038	39.209588
2546.389786	448008.911751	39.214605
2548.718998	448807.418460	39.219623
2551.529729	449597.166703	39.224640
2553.646411	450390.236928	39.229658
2556.878090	451181.828970	39.234676
2559.143378	451976.584994	39.239693
2561.547775	452789.291276	39.244711
2564.279043	453592.151991	39.249728
2566.805596	454400.324959	39.254746
2569.436904	455205.971284	39.259764
2572.502547	456013.081831	39.264781
2574.774087	456824.690406	39.269799
2577.676840	457626.455095	39.274816
2579.946903	458447.403216	39.279834
2582.487842	459255.937779	39.284852
2585.278649	460072.891605	39.289869
2587.793516	460892.739078	39.294887
2590.301713	461714.828689	39.299904
2592.909772	462544.096063	39.304922
2595.828504	463361.601542	39.309940
2598.620658	464194.105238	39.314957
2600.804717	465014.392548	39.319975
2603.930415	465833.630940	39.324992
2606.345550	466654.316570	39.330010
2608.975028	467478.823255	39.335028
2611.578791	468313.860213	39.340045
2614.078945	469140.237387	39.345063
2616.849233	469969.515492	39.350080
2619.323472	470796.431692	39.355098
2621.836597	471622.497125	39.360116
2624.552095	472448.846772	39.365133
2626.880033	473293.360444	39.370151
2629.890086	474115.698334	39.375168
2632.664118	474956.325240	39.380186
2635.175698	475789.330172	39.385204
2637.621793	476620.692199	39.390221
2640.206409	477441.690422	39.395239
2642.850137	478240.116857	39.400256
2645.169566	479051.036343	39.405274
2647.750950	479854.957996	39.410292
2650.295760	480657.335221	39.415309
2652.659484	481460.161295	39.420327
2655.138122	482268.638604	39.425344
2657.761352	483092.253848	39.430362
2660.005540	483917.761919	39.435380
2663.065815	484746.631345	39.440397
2665.350637	485574.883303	39.445415
2667.838173	486421.287349	39.450432
2670.313581	487263.614439	39.455450
2672.896863	488101.542339	39.460468
2675.302203	488965.100985	39.465485
2677.795783	489839.100709	39.470503
2680.707524	490693.001355	39.475520
2683.080461	491570.870497	39.480538
2685.709711	492450.873190	39.485556
2688.603804	493337.448216	39.490573
2690.941934	494226.137922	39.495591
2693.710926	495120.260573	39.500608
2696.396413	496027.215871	39.505626
2698.765660	496933.972946	39.510644
2701.764015	497849.406087	39.515661
2703.912408	498770.983097	39.520679
2707.265385	499702.500243	39.525696
2709.808630	500626.835422	39.530714
2712.469450	501554.327761	39.535732
2715.326206	502481.180966	39.540749
2717.835038	503429.372195	39.545767
2720.971582	504357.031669	39.550784
2723.595230	505296.774972	39.555802
2726.473091	506243.733477	39.560820
2729.503442	507184.913995	39.565837
2731.800870	508136.092793	39.570855
2735.179760	509079.172293	39.575872
2738.186272	510023.215507	39.580890
2740.785321	510968.983968	39.585908
2743.640541	511910.772678	39.590925
2746.357464	512857.266025	39.595943
2749.760318	513805.605418	39.600960
2752.553857	514761.698726	39.605978
2755.156604	515704.410850	39.610996
2758.051779	516642.885734	39.616013
2760.773207	517596.952641	39.621031
2763.585725	518537.946577	39.626048
2766.704504	519486.692014	39.631066
2769.509868	520428.176094	39.636084
2772.686113	521373.571059	39.641101
2774.774540	522320.245355	39.646119
2777.827633	523261.563939	39.651136
2780.800592	524207.319698	39.656154
2783.769365	525150.599412	39.661172
2786.594023	526092.433590	39.666189
2789.033518	527040.767932	39.671207
2791.792071	527981.738531	39.676224
2794.963502	528926.961838	39.681242
2797.710694	529882.415046	39.686260
2800.697413	530822.110139	39.691277
2803.392107	531773.925199	39.696295
2806.067746	532712.040300	39.701312
2809.068227	533650.796494	39.706330
2811.972738	534588.601937	39.711348
2815.127844	535520.517732	39.716365
2818.045121	536471.132944	39.721383
2821.000763	537404.268177	39.726400
2823.574040	538326.084376	39.731418
2826.269092	539261.204454	39.736436
2829.247892	540156.772853	39.741453
2831.842450	541053.404525	39.746471
2834.661421	541939.076607	39.751488
2837.168356	542845.669707	39.756506
2839.851329	543733.816562	39.761524
2842.773781	544629.562642	39.766541
2845.624365	545542.311819	39.771559
2848.721959	546442.187186	39.776576
2851.306355	547353.503392	39.781594
2854.096407	548260.250517	39.786612
2856.999789	549166.215341	39.791629
2859.804473	550092.347077	39.796647
2862.936035	551006.146263	39.801664
2865.614492	551930.967596	39.806682
2868.445236	552858.616210	39.811700
2871.330593	553783.277132	39.816717
2873.885594	554715.467831	39.821735
2876.991590	555651.623911	39.826752
2879.571376	556594.786232	39.831770
2882.257545	557544.949277	39.836788
2885.572154	558490.670219	39.841805
2888.343233	559453.545177	39.846823
2891.212318	560404.327471	39.851840
2894.147011	561368.743860	39.856858
2897.236843	562353.306069	39.861876
2900.129139	563298.098881	39.866893
2902.841687	564277.907461	39.871911
2905.770820	565243.997593	39.876928
2908.519562	566214.263457	39.881946
2911.819195	567204.098159	39.886964
2914.896720	568180.337768	39.891981
2917.691128	569156.198408	39.896999
2920.382643	570138.728185	39.902016
2923.816701	571131.299508	39.907034
2926.577663	572120.792484	39.912052
2929.901718	573102.537122	39.917069
2932.908427	574102.624642	39.922087
2935.232987	575089.247073	39.927104
2938.774889	576073.684519	39.932122
2941.441831	577081.769009	39.937140
2944.658219	578067.306947	39.942157
2947.763631	579071.596016	39.947175
2951.179949	580057.193592	39.952192
2954.163147	581052.564009	39.957210
2956.965742	582059.819482	39.962228
2959.937375	583048.560529	39.967245
2963.336218	584038.855948	39.972263
2965.959468	585039.226384	39.977280
2969.115708	586029.600175	39.982298
2972.023807	587024.746296	39.987316
2975.328821	588016.737286	39.992333
2978.097747	589017.405877	39.997351
2980.730190	590011.447993	40.002368
2984.103739	591006.437793	40.007386
2986.824908	592017.236412	40.012404
2989.852047	593006.353339	40.017421
2993.058968	594014.646728	40.022439
2995.622548	595025.314506	40.027456
2999.004859	596015.873788	40.032474
3001.898832	597026.765550	40.037492
3005.000365	598036.033090	40.042509
3007.654506	599039.277393	40.047527
3010.308625	600049.946224	40.052544
3013.988138	601058.304812	40.057562
3016.747588	602069.380425	40.062580
3019.739746	603079.728015	40.067597
3022.606211	604102.621694	40.072615
3025.726986	605102.307509	40.077632
3028.783491	606081.246130	40.082650
3031.384516	607051.367656	40.087668
3034.293902	608026.509331	40.092685
3037.259835	609000.206472	40.097703
3039.932222	609978.920920	40.102720
3043.026197	610958.431001	40.107738
3045.833040	611954.510117	40.112756
3048.758315	612949.430367	40.117773
3051.812053	613949.441814	40.122791
3054.651948	614945.597621	40.127808
3057.572781	615962.652158	40.132826
3060.399239	616989.428324	40.137844
3063.676339	618000.035794	40.142861
3066.613980	619033.351608	40.147879
3069.648318	620075.401135	40.152896
3072.706894	621103.902045	40.157914
3075.513999	622153.186949	40.162932
3078.513907	623203.687507	40.167949
3081.838553	624260.228004	40.172967
3084.339834	625328.990959	40.177984
3087.742010	626396.149986	40.183002
3090.348104	627475.421852	40.188020
3093.902297	628553.279271	40.193037
3096.755496	629646.674477	40.198055
3099.888235	630740.709592	40.203072
3102.821666	631837.210552	40.208090
3105.804625	632956.754395	40.213108
3109.252655	634051.141928	40.218125
3112.267948	635163.355669	40.223143
3115.304892	636282.035105	40.228160
3118.505363	637390.636107	40.233178
3121.240070	638514.563924	40.238196
3124.870002	639649.547456	40.243213
3127.855442	640776.180672	40.248231
3130.573247	641917.898340	40.253248
3134.253123	643059.180177	40.258266
3137.402507	644196.481713	40.263284
3140.280228	645345.369085	40.268301
3143.686583	646492.393473	40.273319
3146.801341	647655.039448	40.278336
3150.363042	648798.235848	40.283354
3153.365586	649947.474756	40.288372
3156.608030	651106.210202	40.293389
3160.079325	652264.872701	40.298407
3163.230295	653413.886272	40.303424
3166.763186	654566.938050	40.308442
3169.781092	655713.962239	40.313460
3172.841049	656864.680830	40.318477
3176.275621	658031.836316	40.323495
3179.531712	659179.859713	40.328512
3182.683252	660336.528001	40.333530
3185.797393	661500.880684	40.338548
3189.173091	662653.053609	40.343565
3192.459345	663813.415551	40.348583
3195.315108	664974.206053	40.353600
3199.206420	666125.927497	40.358618
3202.147186	667295.379178	40.363636
3205.414484	668453.738656	40.368653
3208.711153	669595.686367	40.373671
3211.922566	670759.294642	40.378688
3215.180654	671911.164709	40.383706
3218.562234	673067.597103	40.388724
3221.740276	674216.114786	40.393741
3224.874832	675376.976084	40.398759
3228.135902	676537.174890	40.403776
3231.591329	677677.516005	40.408794
3234.959069	678832.788115	40.413812
3238.068500	679965.847731	40.418829
3241.310491	681080.314564	40.423847
3244.603889	682179.139136	40.428864
3247.508315	683270.892627	40.433882
3250.472264	684375.020767	40.438900
3253.384270	685480.860841	40.443917
3257.050607	686577.504725	40.448935
3259.829962	687695.558746	40.453952
3263.481113	688808.317080	40.458970
3266.186188	689933.402530	40.463988
3269.324357	691052.022650	40.469005
3272.840751	692183.589810	40.474023
3275.800013	693328.550483	40.479040
3278.937019	694476.608540	40.484058
3282.103731	695629.225132	40.489076
3285.214535	696786.957660	40.494093
3288.427012	697942.042028	40.499111
3291.275331	699119.643539	40.504128
3294.930171	700281.139723	40.509146
3298.047079	701464.578194	40.514164
3301.163581	702663.715439	40.519181
3304.577570	703853.123764	40.524199
3307.725852	705061.289956	40.529216
3311.152524	706264.931223	40.534234
3314.527512	707479.656721	40.539252
3317.606630	708689.504535	40.544269
3320.971198	709909.533243	40.549287
3324.186257	711143.721037	40.554304
3327.580634	712369.284365	40.559322
3330.602875	713615.669306	40.564340
3334.140147	714856.044724	40.569357
3337.608136	716105.205362	40.574375
3340.903610	717361.382611	40.579392
3344.113161	718606.947846	40.584410
3347.647137	719876.954630	40.589428
3350.627947	721135.088970	40.594445
3354.500119	722402.329748	40.599463
3357.927416	723673.602463	40.604480
3361.541950	724946.131243	40.609498
3364.913799	726205.999112	40.614516
3368.330009	727469.421544	40.619533
3371.851804	728739.992908	40.624551
3375.088790	730022.960510	40.629568
3378.872427	731283.162077	40.634586
3382.642390	732568.800056	40.639604
3385.771025	733836.316615	40.644621
3389.240913	735099.973391	40.649639
3392.801270	736387.849711	40.654656
3396.135735	737653.495231	40.659674
3399.466992	738923.480117	40.664692
3402.889004	740203.903943	40.669709
3406.274388	741475.494382	40.674727
3409.606144	742760.748223	40.679744
3413.192882	744032.287936	40.684762
3416.819468	745313.278989	40.689780
3419.800705	746592.441436	40.694797
3423.592182	747872.000132	40.699815
3427.001957	749168.018925	40.704832
3430.564036	750435.957275	40.709850
3433.944780	751728.694723	40.714868
3437.166160	753006.415732	40.719885
3440.967910	754297.864478	40.724903
3443.788073	755578.670955	40.729920
3447.426342	756857.897297	40.734938
3450.982410	758158.580602	40.739956
3454.088640	759447.599229	40.744973
3457.542883	760739.342820	40.749991
3461.294331	762047.642172	40.755008
3464.624903	763308.557953	40.760013
3467.908955	764540.893419	40.765018
3471.014925	765734.257082	40.770023
3474.489104	766842.045642	40.775028
3477.830129	767895.034630	40.780032
3481.108581	768874.115301	40.785037
3484.005838	769802.871978	40.790042
3486.786198	770657.040694	40.795047
3489.788098	771438.857353	40.800052
3492.237998	772153.447149	40.805056
3494.828187	772800.222953	40.810061
3497.621391	773388.992630	40.815066
3499.783510	773898.682996	40.820071
3501.847461	774350.741397	40.825076
3503.409782	774747.657669	40.830080
3505.689719	775094.311265	40.835085
3507.415638	775393.331339	40.840090
3508.820298	775636.611154	40.845095
3510.532817	775825.332649	40.850100
3512.027923	775980.608195	40.855104
3513.341223	776072.649848	40.860109
3514.714378	776149.468518	40.865114
3515.518469	776179.169219	40.870119
3516.995305	776158.692600	40.875124
3518.019187	776134.992163	40.880128
3519.192662	776059.723078	40.885133
3519.925827	775944.747185	40.890138
3520.667480	775808.746064	40.895143
3521.727666	775632.072684	40.900148
3522.015912	775462.808916	40.905152
3522.582564	775257.159510	40.910157
3523.260662	775033.563650	40.915162
3523.783778	774775.962484	40.920167
3524.545367	774520.922722	40.925172
3524.806150	774234.195224	40.930176
3525.018736	773945.691654	40.935181
3525.557706	773635.651485	40.940186
3526.045684	773309.453053	40.945191
3526.139344	772975.424959	40.950196
3526.412791	772641.746092	40.955200
3526.467788	772289.863542	40.960205
3526.891871	771921.648222	40.965210
3527.295972	771552.678895	40.970215
3527.230882	771168.792462	40.975220
3527.045379	770789.980265	40.980224
3527.022904	770395.750105	40.985229
3527.288498	770001.451462	40.990234
3527.125445	769606.266250	40.995239
3527.568831	769210.762926	41.000244
3527.692375	768800.753968	41.005248
3527.368162	768380.594847	41.010253
3527.530005	767971.026579	41.015258
3527.922273	767547.794546	41.020263
3527.625118	767129.433173	41.025268
3526.953896	766714.708300	41.030272
3527.454298	766282.464593	41.035277
3526.984820	765862.581659	41.040282
3526.854339	765442.224853	41.045287
3526.913829	765026.053245	41.050292
3526.748245	764603.682958	41.055296
3526.753619	764189.150185	41.060301
3526.727869	763773.761323	41.065306
3526.596571	763349.095684	41.070311
3526.738167	762927.418771	41.075316
3526.459601	762507.365701	41.080320
3526.339615	762088.101554	41.085325
3526.324781	761659.770120	41.090330
3525.896300	761249.980760	41.095335
3526.248373	760810.885712	41.100340
3525.917660	760405.178250	41.105344
3525.762497	759980.425432	41.110349
3525.752531	759570.525415	41.115354
3525.265892	759159.694930	41.120359
3525.491388	758730.121810	41.125364
3525.370237	758329.943388	41.130368
3525.259813	757903.389082	41.135373
3525.351446	757500.911210	41.140378
3524.784030	757089.340519	41.145383
3524.667217	756676.390036	41.150388
3524.510302	756273.246639	41.155392
3524.236454	755876.123575	41.160397
3524.249316	755473.453002	41.165402
3524.021758	755079.687210	41.170407
3523.978298	754667.307257	41.175412
3523.399176	754280.025926	41.180416
3523.007657	753888.744025	41.185421
3523.107446	753496.126757	41.190426
3522.795816	753126.865182	41.195431
3523.006635	752729.005432	41.200436
3522.967298	752358.723846	41.205440
3522.397574	751982.041971	41.210445
3522.283947	751605.760449	41.215450
3522.315097	751242.674135	41.220455
3522.347040	750856.502865	41.225460
3521.771624	750492.048764	41.230464
3521.689744	750124.828554	41.235469
3521.473406	749768.629892	41.240474
3521.567973	749406.138612	41.245479
3521.279510	749034.454351	41.250484
3521.047478	748692.240532	41.255488
3521.200987	748329.936361	41.260493
3521.175534	747971.943835	41.265498
3520.533759	747627.378807	41.270503
3521.017438	747273.025905	41.275508
3520.283467	746921.180322	41.280512
3520.196350	746572.029394	41.285517
3519.893497	746233.920211	41.290522
3519.635860	745909.282572	41.295527
3519.633654	745565.064818	41.300532
3519.247146	745242.991100	41.305536
3518.911818	744909.674321	41.310541
3519.290706	744578.549158	41.315546
3518.892496	744269.636663	41.320551
3519.131151	743933.464783	41.325556
3518.688319	743621.617221	41.330560
3518.439012	743310.170396	41.335565
3518.443263	742982.302999	41.340570
3518.253393	742677.150373	41.345575
3518.323239	742365.514714	41.350580
3517.924104	742064.872775	41.355584
3518.089836	741756.559962	41.360589
3517.810974	741439.604263	41.365594
3517.298481	741149.381205	41.370599
3517.232145	740846.165206	41.375604
3517.162448	740571.229700	41.380608
3516.960159	740261.385983	41.385613
3516.768161	739968.939957	41.390618
3516.604414	739692.802339	41.395623
3516.750242	739406.809462	41.400628
3516.623655	739133.812232	41.405632
3516.076389	738840.443263	41.410637
3516.050444	738564.540561	41.415642
3515.637900	738297.300624	41.420647
3515.952911	738024.736801	41.425652
3515.864254	737760.245642	41.430656
3515.316454	737500.027150	41.435661
3515.410813	737236.824435	41.440666
3515.360847	736975.764598	41.445671
3515.126317	736707.600855	41.450676
3515.065127	736443.952295	41.455680
3514.831242	736197.347336	41.460685
3514.762649	735938.384684	41.465690
3514.582662	735694.378294	41.470695
3514.068642	735445.371284	41.475700
3514.336926	735198.207393	41.480704
3513.862365	734962.245286	41.485709
3514.131221	734711.601639	41.490714
3513.905713	734483.008958	41.495719
3513.959123	734242.335353	41.500724
3513.771318	734008.871989	41.505728
3513.418268	733774.637035	41.510733
3513.451968	733541.618647	41.515738
3513.062958	733318.762315	41.520743
3513.044371	733099.650816	41.525748
3512.676158	732891.334260	41.530752
3512.529721	732671.291535	41.535757
3512.846604	732452.057665	41.540762
3512.726686	732243.435920	41.545767
3512.346207	732023.661678	41.550772
3512.385183	731814.656090	41.555776
3512.379407	731598.670708	41.560781
3512.313826	731394.920215	41.565786
3512.084656	731195.400631	41.570791
3512.175921	730983.591933	41.575796
3511.891512	730777.633579	41.580800
3512.013105	730580.616162	41.585805
3511.829741	730371.461415	41.590810
3511.651048	730168.293016	41.595815
3511.444144	729967.699540	41.600820
3511.430391	729787.969774	41.605824
3511.331486	729597.155728	41.610829
3511.651644	729394.182949	41.615834
3511.260214	729207.667511	41.620839
3511.407702	729008.973219	41.625844
3511.174229	728823.165922	41.630848
3510.953608	728637.154132	41.635853
3510.671327	728449.860339	41.640858
3510.873264	728272.191592	41.645863
3510.822133	728092.925941	41.650868
3510.679167	727905.844390	41.655872
3510.549619	727731.091728	41.660877
3510.455084	727542.804929	41.665882
3510.361047	727379.235105	41.670887
3510.478002	727201.656163	41.675892
3510.120667	727027.173701	41.680896
3510.243964	726848.149269	41.685901
3510.155166	726674.358211	41.690906
3510.020165	726512.115548	41.695911
3509.975425	726345.048640	41.700916
3510.033463	726187.177512	41.705920
3509.977495	726010.344473	41.710925
3509.944425	725840.292353	41.715930
3509.233449	725695.124444	41.720935
3509.619126	725524.154391	41.725940
3509.561896	725365.890035	41.730944
3509.143577	725210.011212	41.735949
3509.359589	725052.488675	41.740954
3509.068256	724905.701428	41.745959
3509.251133	724749.070562	41.750964
3508.776202	724593.734516	41.755968
3508.991700	724440.908425	41.760973
3508.871632	724296.213145	41.765978
3508.679307	724157.474580	41.770983
3508.641796	724012.116410	41.775988
3508.738413	723874.168021	41.780992
3508.442416	723730.532620	41.785997
3508.551304	723575.626376	41.791002
3508.417446	723452.479194	41.796007
3508.223519	723307.679605	41.801012
3508.188861	723172.368133	41.806016
3508.120173	723036.366100	41.811021
3507.986518	722896.258324	41.816026
3507.684169	722771.393840	41.821031
3507.850404	722645.855414	41.826036
3507.544367	722527.233709	41.831040
3507.427094	722403.126304	41.836045
3508.069829	722272.100366	41.841050
3507.557298	722150.235492	41.846055
3507.485717	722017.637742	41.851060
3507.229554	721903.460544	41.856064
3507.155231	721777.304115	41.861069
3507.286089	721658.994582	41.866074
3507.345464	721538.612908	41.871079
3507.445615	721422.089825	41.876084
3507.375406	721301.131126	41.881088
3507.517149	721183.308800	41.886093
3507.375488	721057.945793	41.891098
3506.996692	720948.336992	41.896103
3507.196860	720835.061500	41.901108
3507.156321	720721.724965	41.906112
3506.809750	720593.661713	41.911117
3507.036323	720480.872870	41.916122
3507.443403	720366.614820	41.921127
3506.807110	720253.320483	41.926132
3506.633126	720146.890359	41.931136
3506.692173	720038.437040	41.936141
3506.829736	719919.109909	41.941146
3506.421943	719837.110928	41.946151
3506.574715	719717.927170	41.951156
3506.794249	719612.863422	41.956160
3506.633789	719512.720692	41.961165
3506.884361	719401.450535	41.966170
3506.691098	719298.434434	41.971175
3506.606267	719198.325055	41.976180
3506.710049	719083.157159	41.981184
3506.062311	718969.252131	41.986189
3506.391400	718879.435496	41.991194
3506.267457	718781.112896	41.996199
3506.304071	718673.339824	42.001204
3506.036743	718579.353153	42.006208
3506.059639	718490.078733	42.011213
3506.148027	718398.560763	42.016218
3506.158658	718288.356819	42.021223
3506.137785	718195.515531	42.026228
3505.948422	718107.164741	42.031232
3505.882203	718012.493789	42.036237
3506.054900	717914.062509	42.041242
3505.853207	717830.025893	42.046247
3505.867268	717726.708246	42.051252
3505.975894	717653.183434	42.056256
3505.444103	717550.399957	42.061261
3505.730578	717461.467933	42.066266
3505.515157	717375.048152	42.071271
3505.695863	717289.951068	42.076276
3505.884295	717198.701108	42.081280
3505.400568	717104.733526	42.086285
3505.707520	717021.349029	42.091290
3505.531818	716949.204196	42.096295
3505.449529	716857.003043	42.101300
3505.647344	716773.088411	42.106304
3505.140008	716690.727703	42.111309
3505.499808	716605.643773	42.116314
3505.067450	716532.793556	42.121319
3505.080961	716439.778326	42.126324
3505.123012	716364.913795	42.131328
3504.831695	716300.422015	42.136333
3505.043286	716213.919906	42.141338
3504.888122	716144.294806	42.146343
3504.947824	716080.239584	42.151348
3504.949937	716007.759702	42.156352
3504.879616	715926.162845	42.161357
3505.069905	715845.812132	42.166362
3504.735303	715775.717439	42.171367
3504.885182	715694.875831	42.176372
3504.595613	715630.676292	42.181376
3504.589012	715560.624981	42.186381
3504.963481	715486.293201	42.191386
3504.835202	715415.119634	42.196391
3504.730455	715334.415750	42.201396
3504.991914	715266.401598	42.206400
3504.844261	715200.091593	42.211405
3505.037297	715130.599184	42.216410
3504.736550	715069.622177	42.221415
3505.025329	714982.747391	42.226420
3505.115386	714917.437923	42.231424
3504.865396	714832.783868	42.236429
3504.813509	714761.790660	42.241434
3504.520939	714688.752576	42.246439
3504.742121	714620.045203	42.251444
3504.674305	714549.350539	42.256448
3504.787301	714484.877454	42.261453
3504.917204	714405.564954	42.266458
3504.754811	714354.731914	42.271463
3504.881842	714270.952864	42.276468
3504.756071	714207.410165	42.281472
3504.906985	714146.550538	42.286477
3504.897208	714064.330226	42.291482
3504.612219	714001.358046	42.296487
3504.563582	713921.524584	42.301492
3504.521347	713854.194183	42.306496
3504.248481	713779.060834	42.311501
3504.620652	713714.737657	42.316506
3504.695836	713662.819214	42.321511
3504.408187	713588.530208	42.326516
3504.635749	713526.809881	42.331520
3504.179098	713460.735621	42.336525
3504.501565	713392.696328	42.341530
3503.945837	713335.669193	42.346535
3504.391107	713264.432601	42.351540
3504.171241	713216.430858	42.356544
3503.965544	713161.329917	42.361549
3504.522507	713086.748448	42.366554
3504.109110	713027.958840	42.371559
3504.175267	712970.777141	42.376564
3504.164370	712913.111474	42.381568
3504.127086	712862.447354	42.386573
3504.509949	712787.147515	42.391578
3503.810828	712743.291615	42.396583
3504.216213	712687.094313	42.401588
3504.312656	712624.843099	42.406592
3504.181435	712560.743001	42.411597
3504.460165	712498.560083	42.416602
3504.231361	712443.855325	42.421607
3504.062367	712377.228896	42.426612
3504.185155	712320.777949	42.431616
3504.116718	712259.841643	42.436621
3504.194240	712207.318313	42.441626
3503.653660	712144.324796	42.446631
3504.163153	712085.823265	42.451636
3504.253007	712030.616637	42.456640
3503.826737	711984.478352	42.461645
3503.996102	711922.110700	42.466650
3504.025704	711875.251462	42.471655
3504.223809	711813.424252	42.476660
3504.174265	711755.211103	42.481664
3503.821857	711696.104395	42.486669
3504.003865	711632.541292	42.491674
3503.376841	711586.235379	42.496679
3503.677116	711539.081507	42.501684
3503.644544	711486.174771	42.506688
3503.464898	711434.383948	42.511693
3503.847195	711385.081331	42.516698
3503.630453	711340.840859	42.521703
3503.755521	711282.893526	42.526708
3503.664419	711233.767315	42.531712
3503.548161	711192.388506	42.536717
3503.535503	711143.596314	42.541722
3503.538227	711098.276011	42.546727
3503.741878	711049.596553	42.551732
3503.670069	711001.607517	42.556736
3503.360412	710953.161009	42.561741
3503.720180	710908.277255	42.566746
3503.634832	710863.168771	42.571751
3503.639058	710806.429467	42.576756
3503.990679	710762.787297	42.581760
3503.590427	710718.375264	42.586765
3503.744641	710657.738269	42.591770
3503.797034	710617.818110	42.596775
3503.904319	710560.365205	42.601780
3503.981702	710499.888673	42.606784
3503.714288	710456.992291	42.611789
3503.679760	710393.008835	42.616794
3503.530653	710353.070996	42.621799
3503.465409	710300.360847	42.626804
3503.469010	710258.610245	42.631808
3503.397591	710215.581063	42.636813
3503.510365	710166.464744	42.641818
3503.593216	710117.948805	42.646823
3503.782543	710073.336966	42.651828
3503.822756	710019.217653	42.656832
3503.469483	709975.141516	42.661837
3503.822906	709926.480613	42.666842
3503.433329	709891.693715	42.671847
3503.621142	709835.662383	42.676852
3503.739630	709781.479018	42.681856
3503.510868	709732.267541	42.686861
3503.580610	709675.857444	42.691866
3503.237443	709634.756694	42.696871
3503.575786	709597.515232	42.701876
3503.403221	709549.038148	42.706880
3503.192702	709514.964922	42.711885
3503.405286	709454.706944	42.716890
3503.229697	709426.486090	42.721895
3503.348669	709370.264456	42.726900
3503.336909	709329.256571	42.731904
3503.050456	709291.371998	42.736909
3503.404137	709247.870698	42.741914
3503.305472	709216.409264	42.746919
3503.269056	709166.715986	42.751924
3503.566624	709118.109337	42.756928
3503.293965	709086.427846	42.761933
3503.241771	709033.211219	42.766938
3503.035425	709002.610803	42.771943
3503.100939	708954.240065	42.776948
3503.259717	708914.443366	42.781952
3503.024151	708874.562507	42.786957
3503.380322	708841.982065	42.791962
3503.166242	708795.344660	42.796967
3503.105220	708747.341167	42.801972
3503.206223	708706.262061	42.806977
3503.109406	708675.592774	42.811981
3502.963513	708638.625547	42.816986
3502.980142	708616.974179	42.821991
3503.139527	708563.521155	42.826996
3503.468203	708530.149605	42.832001
3503.290590	708488.668485	42.837005
3503.194780	708435.902215	42.842010
3503.197647	708394.937096	42.847015
3503.019290	708362.095331	42.852020
3503.108312	708319.576365	42.857025
3503.123179	708286.553506	42.862029
3502.973001	708233.546674	42.867034
3503.066548	708205.724339	42.872039
3503.150521	708166.284079	42.877044
3503.223743	708123.866057	42.882049
3502.818954	708084.704585	42.887053
3502.989190	708055.627723	42.892058
3502.908985	708022.321575	42.897063
3503.050233	707977.408795	42.902068
3503.222651	707943.067577	42.907073
3502.912569	707904.088300	42.912077
3503.148609	707857.272299	42.917082
3503.081255	707830.617382	42.922087
3503.016196	707800.485961	42.927092
3503.316326	707744.074829	42.932097
3502.926983	707706.001558	42.937101
3503.191344	707672.438640	42.942106
3503.147439	707637.684920	42.947111
3503.372804	707599.857495	42.952116
3503.536060	707559.805477	42.957121
3503.259314	707511.135380	42.962125
3503.483179	707459.253953	42.967130
3503.340760	707429.431936	42.972135
3502.970992	707383.905019	42.977140
3503.233809	707354.313926	42.982145
3502.836562	707316.786491	42.987149
3502.941655	707263.632280	42.992154
3503.102784	707233.660241	42.997159
3503.241613	707190.779848	43.002164
3503.271709	707151.989404	43.007169
3503.108429	707119.488026	43.012173
3503.367408	707062.731572	43.017178
3503.359314	707031.843136	43.022183
3503.093855	706997.421307	43.027188
3503.290170	706959.198552	43.032193
3503.194195	706923.010305	43.037197
3503.196382	706881.442119	43.042202
3503.170784	706840.176292	43.047207
3503.126219	706801.197914	43.052212
3502.987770	706767.648179	43.057217
3503.137650	706725.657594	43.062221
3503.438526	706686.075469	43.067226
3502.951028	706649.453944	43.072231
3503.209878	706610.524034	43.077236
3503.197227	706566.622535	43.082241
3502.930281	706524.004343	43.087245
3503.012886	706487.288184	43.092250
3502.760775	706457.133209	43.097255
3503.284069	706414.930581	43.102260
3503.117252	706377.013407	43.107265
3503.118894	706337.578322	43.112269
3503.624718	706300.294965	43.117274
3502.772335	706262.390923	43.122279
3502.558823	706238.735150	43.127284
3502.953649	706193.622268	43.132289
3502.992031	706167.093768	43.137293
3503.134046	706126.243903	43.142298
3503.155654	706087.251388	43.147303
3503.131184	706050.153669	43.152308
3502.833260	706010.716783	43.157313
3503.115185	705990.703795	43.162317
3503.108254	705953.155754	43.167322
3503.019201	705911.051566	43.172327
3503.107731	705874.828508	43.177332
3503.120521	705833.849545	43.182337
3502.765853	705788.957389	43.187341
3502.944135	705746.709007	43.192346
3503.159262	705727.004434	43.197351
3503.341400	705681.526565	43.202356
3503.296083	705636.830991	43.207361
3503.016724	705596.693765	43.212365
3503.154604	705561.454669	43.217370
3502.913655	705522.552537	43.222375
3502.673221	705483.848828	43.227380
3503.070153	705456.116623	43.232385
3503.075319	705424.077797	43.237389
3503.096868	705383.542295	43.242394
3502.935952	705355.951364	43.247399
3502.640605	705323.713325	43.252404
3502.938940	705285.366995	43.257409
3502.816043	705255.683243	43.262413
3503.047505	705198.819707	43.267418
3502.955795	705182.293838	43.272423
3503.137236	705138.849813	43.277428
3502.994144	705102.214622	43.282433
3503.066699	705071.256196	43.287437
3502.931828	705027.714715	43.292442
3502.632917	704999.897015	43.297447
3502.726631	704958.105777	43.302452
3502.917673	704932.442462	43.307457
3502.762384	704894.367844	43.312461
3502.999302	704864.176384	43.317466
3502.775900	704832.322051	43.322471
3502.608012	704794.398093	43.327476
3502.804895	704760.536911	43.332481
3502.660523	704736.617245	43.337485
3503.022122	704688.620807	43.342490
3502.765239	704671.574744	43.347495
3502.792193	704630.687089	43.352500
3502.938854	704605.328173	43.357505
3503.003021	704563.241838	43.362509
3502.813397	704527.555730	43.367514
3502.888316	704499.873525	43.372519
3502.756210	704473.367916	43.377524
3502.907915	704435.141334	43.382529
3502.861519	704409.714303	43.387533
3503.024595	704366.666846	43.392538
3502.882836	704330.624294	43.397543
3502.468933	704298.749707	43.402548
3502.816679	704262.924280	43.407553
3502.994840	704228.368608	43.412557
3503.098673	704193.775368	43.417562
3502.928029	704168.517138	43.422567
3502.958943	704122.608881	43.427572
3502.937875	704107.460325	43.432577
3502.601354	704062.506519	43.437581
3503.032072	704013.948482	43.442586
3503.015576	703993.831015	43.447591
3503.043779	703953.337392	43.452596
3503.067025	703919.700255	43.457601
3502.833837	703886.999489	43.462605
3503.025009	703840.566527	43.467610
3502.946369	703817.627099	43.472615
3503.168134	703778.392461	43.477620
3503.198170	703741.325529	43.482625
3502.890609	703715.840134	43.487629
3503.314563	703676.223948	43.492634
3502.825654	703642.073950	43.497639
3502.718412	703607.612515	43.502644
3502.925479	703564.851918	43.507649
3502.852137	703536.495516	43.512653
3502.931195	703505.480737	43.517658
3502.933066	703466.678385	43.522663
3502.811645	703429.535712	43.527668
3503.250970	703401.243438	43.532673
3502.950784	703363.931209	43.537677
3503.047829	703328.192918	43.542682
3503.130073	703293.003440	43.547687
3503.359965	703247.008075	43.552692
3503.175405	703207.241604	43.557697
3502.832258	703167.103607	43.562701
3502.983737	703133.790083	43.567706
3502.918057	703101.009063	43.572711
3502.921898	703072.936536	43.577716
3502.935794	703034.527750	43.582721
3503.081959	702993.264929	43.587725
3502.990878	702951.295722	43.592730
3502.832130	702933.484776	43.597735
3502.649850	702896.797022	43.602740
3502.895739	702859.541697	43.607745
3502.815530	702832.774085	43.612749
3502.757255	702794.326442	43.617754
3503.106311	702753.575603	43.622759
3502.821675	702720.133610	43.627764
3503.135876	702687.785303	43.632769
3502.949871	702656.413672	43.637773
3503.064555	702620.073314	43.642778
3502.979788	702586.498496	43.647783
3502.816954	702544.837275	43.652788
3503.268710	702515.993509	43.657793
3503.081282	702480.248919	43.662797
3503.150342	702435.319217	43.667802
3502.937832	702409.168364	43.672807
3502.856261	702356.710383	43.677812
3502.821298	702322.778516	43.682817
3502.738747	702293.028271	43.687821
3502.830998	702251.820507	43.692826
3502.562693	702231.839829	43.697831
3502.545540	702196.066011	43.702836
3502.637279	702164.448077	43.707841
3502.503905	702135.947923	43.712845
3502.575961	702110.643706	43.717850
3503.153909	702079.988846	43.722855
3502.911872	702053.841789	43.727860
3503.043767	702012.974197	43.732865
3502.757147	701986.784594	43.737869
3503.104907	701949.955810	43.742874
3502.849769	701907.412300	43.747879
3502.923962	701881.808916	43.752884
3502.870305	701846.486903	43.757889
3502.714839	701823.703942	43.762893
3502.985254	701784.551676	43.767898
3502.858666	701754.260230	43.772903
3502.918460	701720.757634	43.777908
3503.004822	701685.859131	43.782913
3502.596289	701654.669634	43.787917
3502.929098	701618.289151	43.792922
3502.572946	701576.307294	43.797927
3502.837734	701545.354307	43.802932
3502.934030	701515.323465	43.807937
3502.699436	701474.960985	43.812941
3502.947576	701446.047847	43.817946
3502.897640	701420.761729	43.822951
3502.950472	701389.644339	43.827956
3503.051023	701349.573914	43.832961
3502.759584	701314.686486	43.837965
3502.794504	701282.627461	43.842970
3502.905339	701247.872258	43.847975
3502.509548	701213.051314	43.852980
3502.638967	701180.181211	43.857985
3502.415365	701158.103476	43.862989
3502.810291	701125.239112	43.867994
3502.698740	701099.266469	43.872999
3502.817255	701071.814642	43.878004
3502.697786	701039.879559	43.883009
3502.651291	700997.297222	43.888013
3502.621091	700979.659878	43.893018
3502.439323	700951.014730	43.898023
3502.494002	700922.976590	43.903028
3502.802710	700880.335152	43.908033
3502.934377	700860.384809	43.913037
3502.729543	700826.524805	43.918042
3502.677940	700797.559518	43.923047
3502.728033	700758.836541	43.928052
3502.866037	700727.653058	43.933057
3502.768671	700693.576036	43.938061
3502.932113	700651.603500	43.943066
3502.898530	700636.152766	43.948071
3502.505334	700592.830405	43.953076
3502.622842	700568.210011	43.958081
3502.873100	700550.127991	43.963085
3503.089233	700503.424621	43.968090
3502.714534	700468.646926	43.973095
3502.420295	700445.187431	43.978100
3502.785815	700417.692848	43.983105
3502.847931	700386.222452	43.988109
3502.909678	700356.292718	43.993114
3503.017985	700324.715088	43.998119
3502.676624	700298.529428	44.003124
3503.027848	700272.776273	44.008129
3502.480161	700231.366210	44.013133
3502.728980	700188.035450	44.018138
3502.772737	700174.261002	44.023143
3502.697101	700129.790582	44.028148
3503.000267	700093.259533	44.033153
3502.671584	700075.619847	44.038157
3502.920733	700027.218625	44.043162
3502.682577	700000.418636	44.048167
3502.635874	699960.763727	44.053172
3502.915211	699944.663774	44.058177
3502.906272	699913.750118	44.063181
3502.629720	699854.350797	44.068186
3502.938833	699840.482395	44.073191
3502.579375	699805.798956	44.078196
3503.259312	699761.997418	44.083201
3502.711727	699739.373034	44.088205
3503.118877	699716.392452	44.093210
3502.689685	699681.570898	44.098215
3502.941886	699647.481899	44.103220
3502.879360	699618.415096	44.108225
3502.653221	699579.285074	44.113229
3503.168184	699541.523909	44.118234
3502.832601	699523.238077	44.123239
3503.004145	699472.908079	44.128244
3502.756360	699453.514113	44.133249
3502.734659	699425.284937	44.138253
3502.659145	699390.751885	44.143258
3502.699293	699363.506436	44.148263
3502.834078	699319.891937	44.153268
3503.010932	699288.945461	44.158273
3502.629697	699255.257556	44.163277
3502.867514	699224.350513	44.168282
3502.699861	699190.975114	44.173287
3502.649469	699149.726515	44.178292
3502.894008	699126.920308	44.183297
3502.915272	699106.735628	44.188301
3502.575311	699062.104510	44.193306
3502.744596	699037.073619	44.198311
3502.634196	698999.562297	44.203316
3502.688680	698964.310229	44.208321
3502.256630	698940.024360	44.213325
3502.737715	698910.815923	44.218330
3502.865474	698879.478424	44.223335
3502.763230	698851.161253	44.228340
3502.793611	698818.795694	44.233345
3502.579053	698797.058466	44.238349
3502.646694	698763.095864	44.243354
3502.612981	698731.187929	44.248359
3502.687026	698702.542972	44.253364
3502.755704	698677.129954	44.258369
3502.533176	698643.960356	44.263373
3502.834795	698618.260233	44.268378
3502.815069	698585.404967	44.273383
3502.644905	698557.793989	44.278388
3502.922650	698520.266369	44.283393
3502.863793	698498.701588	44.288397
3502.643036	698448.480071	44.293402
3502.756004	698418.982683	44.298407
3502.513473	698384.771460	44.303412
3502.738688	698367.733017	44.308417
3502.830884	698326.606188	44.313421
3502.980915	698298.096527	44.318426
3502.897083	698280.412871	44.323431
3502.727943	698228.391949	44.328436
3502.887183	698191.479004	44.333441
3502.764556	698169.227944	44.338445
3502.710645	698126.782009	44.343450
3502.761229	698114.743161	44.348455
3502.583272	698077.388170	44.353460
3502.885040	698029.911818	44.358465
3502.593103	698007.539107	44.363469
3502.811221	697985.579429	44.368474
3502.827390	697962.012411	44.373479
3502.683764	697926.192255	44.378484
3502.700846	697890.792901	44.383489
3502.361345	697859.180760	44.388493
3502.648463	697819.858882	44.393498
3502.743088	697806.072335	44.398503
3502.689795	697780.975117	44.403508
3502.639342	697754.187041	44.408513
3502.703025	697722.955409	44.413517
3502.617434	697685.732679	44.418522
3502.760118	697659.210783	44.423527
3502.467824	697630.523268	44.428532
3502.399284	697582.160921	44.433537
3502.895500	697563.982512	44.438541
3502.799222	697525.319092	44.443546
3502.767127	697501.410779	44.448551
3502.547357	697480.715199	44.453556
3503.082832	697440.604953	44.458561
3502.958854	697414.523997	44.463565
3502.948258	697370.774632	44.468570
3502.861016	697343.891936	44.473575
3503.085643	697311.091079	44.478580
3502.843145	697273.892464	44.483585
3502.609808	697237.835698	44.488589
3503.029865	697196.599846	44.493594
3502.708772	697174.975594	44.498599
3502.684841	697147.186932	44.503604
3502.923045	697106.875562	44.508609
3502.494382	697075.175856	44.513613
3502.489659	697043.754212	44.518618
3502.759747	697027.948767	44.523623
3502.849144	696989.103240	44.528628
3503.088490	696963.060516	44.533633
3502.610104	696923.761346	44.538637
3502.862653	696888.816363	44.543642
3502.651564	696862.151484	44.548647
3502.694401	696837.035735	44.553652
3502.796698	696795.949814	44.558657
3502.815417	696774.069699	44.563661
3502.466964	696737.085158	44.568666
3502.627836	696705.535580	44.573671
3502.609387	696679.236174	44.578676
3502.607664	696645.227109	44.583681
3502.533132	696624.555304	44.588685
3502.691065	696585.050324	44.593690
3502.519144	696568.919120	44.598695
3502.544891	696537.043153	44.603700
3502.515371	696499.110061	44.608705
3502.328482	696468.760555	44.613709
3502.656728	696447.773353	44.618714
3502.725318	696420.862163	44.623719
3502.726167	696389.486994	44.628724
3503.062279	696352.338311	44.633729
3502.736428	696330.414430	44.638733
3502.648017	696292.241537	44.643738
3502.314794	696256.346386	44.648743
3502.332222	696229.890557	44.653748
3502.600625	696190.514781	44.658753
3502.599798	696188.128230	44.663757
3502.565374	696148.155753	44.668762
3502.481461	696122.760513	44.673767
3502.215299	696101.174296	44.678772
3502.368317	696084.789763	44.683777
3502.419513	696050.272441	44.688781
3502.701901	696024.319309	44.693786
3502.716729	696000.498645	44.698791
3502.477575	695978.808228	44.703796
3502.413928	695939.684953	44.708801
3502.557223	695914.848380	44.713805
3502.673137	695876.640022	44.718810
3502.585012	695860.891521	44.723815
3502.347071	695839.648095	44.728820
3502.638303	695799.968463	44.733825
3502.938173	695774.956518	44.738829
3502.872193	695736.429444	44.743834
3502.730285	695708.456788	44.748839
3502.669367	695675.647187	44.753844
3502.949041	695635.521181	44.758849
3502.590817	695619.220031	44.763853
3502.642641	695579.181042	44.768858
3502.372781	695554.709905	44.773863
3502.432392	695523.769528	44.778868
3502.763065	695496.165877	44.783873
3502.409572	695485.433226	44.788877
3502.448667	695460.761733	44.793882
3502.606919	695424.036289	44.798887
3502.393835	695395.825730	44.803892
3502.448940	695372.692938	44.808897
3502.478884	695340.662780	44.813901
3502.358255	695308.856235	44.818906
3502.501387	695274.469924	44.823911
3502.761398	695258.911629	44.828916
3502.693399	695230.626906	44.833921
3502.957746	695211.437566	44.838925
3502.699175	695174.431666	44.843930
3502.865039	695145.113539	44.848935
3502.758804	695113.701760	44.853940
3502.764965	695072.971786	44.858945
3502.505087	695048.398142	44.863949
3502.481027	695015.580021	44.868954
3502.647442	694979.547619	44.873959
3502.527089	694961.366015	44.878964
3502.597210	694922.663779	44.883969
3502.624622	694896.102856	44.888973
3502.531781	694861.704098	44.893978
3502.476836	694844.008790	44.898983
3502.340483	694815.783738	44.903988
3502.601229	694791.272784	44.908993
3502.168489	694760.858462	44.913997
3502.586702	694723.391030	44.919002
3502.476829	694715.452035	44.924007
3502.109340	694684.131515	44.929012
3502.759368	694667.015941	44.934017
3502.854804	694632.734467	44.939021
3502.668201	694617.298376	44.944026
3502.977639	694584.970768	44.949031
3502.706909	694553.981974	44.954036
3502.619598	694518.387375	44.959041
3502.482421	694490.758225	44.964045
3502.675338	694448.204199	44.969050
3502.545099	694429.326859	44.974055
3502.514486	694395.662047	44.979060
3502.565679	694367.354929	44.984065
3502.248605	694345.524142	44.989069
3502.582194	694309.909083	44.994074
3502.665280	694273.439935	44.999079
3502.343011	694250.664809	45.004084
3502.933028	694219.334070	45.009089
3502.406624	694202.510932	45.014093
3502.399748	694170.432880	45.019098
3502.686965	694149.894624	45.024103
3502.609339	694116.932799	45.029108
3502.965057	694083.053933	45.034113
3502.523929	694057.512689	45.039117
3502.640909	694024.220036	45.044122
3502.562826	694002.398758	45.049127
3502.486584	693967.993799	45.054132
3502.651402	693935.687661	45.059137
3502.823269	693913.924452	45.064141
3502.788607	693869.415683	45.069146
3502.914445	693854.374412	45.074151
3502.616348	693826.322076	45.079156
3502.872505	693792.110348	45.084161
3502.677132	693771.352317	45.089165
3502.468421	693734.232713	45.094170
3502.618887	693702.773637	45.099175
3502.578954	693665.924363	45.104180
3502.754048	693625.557816	45.109185
3502.513243	693629.228466	45.114189
3502.334009	693591.854718	45.119194
3502.738347	693551.897708	45.124199
3502.512591	693534.725325	45.129204
3502.922228	693511.230828	45.134209
3502.699842	693471.973602	45.139213
3502.499879	693434.005735	45.144218
3502.761165	693410.634897	45.149223
3502.897738	693381.614216	45.154228
3502.671095	693340.317780	45.159233
3502.638475	693313.612797	45.164237
3502.427110	693281.167311	45.169242
3502.840766	693251.254961	45.174247
3502.746437	693234.458265	45.179252
3502.950476	693198.561665	45.184257
3502.416086	693156.618716	45.189261
3502.602649	693125.649063	45.194266
3502.411709	693092.950819	45.199271
3502.503937	693079.853692	45.204276
3502.466796	693053.795314	45.209281
3502.358335	693038.492824	45.214285
3502.312563	693000.696666	45.219290
3502.669157	692981.487317	45.224295
3502.510939	692950.474386	45.229300
3502.598419	692921.062357	45.234305
3502.460178	692892.433564	45.239309
3502.309404	692876.590600	45.244314
3502.466788	692837.914650	45.249319
3502.338233	692820.078212	45.254324
3502.397459	692779.925898	45.259329
3502.269004	692767.163136	45.264333
3502.467989	692741.860827	45.269338
3502.504398	692726.484185	45.274343
3502.320788	692691.495060	45.279348
3502.696210	692663.676274	45.284353
3502.387047	692633.781476	45.289357
3502.381247	692608.562278	45.294362
3502.649102	692572.951109	45.299367
3502.482003	692565.517063	45.304372
3502.587240	692531.076643	45.309377
3502.615492	692508.139798	45.314381
3502.563217	692477.256995	45.319386
3502.543674	692454.576612	45.324391
3502.324117	692421.482658	45.329396
3502.445327	692400.719005	45.334401
3501.928241	692370.111405	45.339405
3502.489728	692349.673045	45.344410
3502.487850	692312.961139	45.349415
3502.318292	692286.723356	45.354420
3502.390870	692267.808005	45.359425
3502.087969	692254.874270	45.364429
3502.267687	692231.663025	45.369434
3502.348743	692203.493343	45.374439
3502.366174	692191.402165	45.379444
3502.641166	692167.180125	45.384449
3502.298451	692150.571554	45.389453
3502.150523	692110.500109	45.394458
3502.235966	692086.458324	45.399463
3502.035943	692061.319331	45.404468
3502.424328	692035.735077	45.409473
3502.151277	692023.940275	45.414477
3502.191316	691992.941089	45.419482
3502.424183	691979.321697	45.424487
3502.174781	691953.245332	45.429492
3502.299554	691934.917648	45.434497
3502.192647	691918.568274	45.439501
3502.156497	691886.437070	45.444506
3502.401877	691869.532074	45.449511
3502.403703	691836.349720	45.454516
3502.347227	691811.833099	45.459521
3502.381655	691789.987859	45.464525
3502.444650	691768.287104	45.469530
3502.539343	691738.720745	45.474535
3502.018108	691725.175482	45.479540
3502.414910	691691.081769	45.484545
3502.418785	691669.490016	45.489549
3502.559706	691648.572119	45.494554
3502.646591	691611.245708	45.499559
3502.464094	691583.714499	45.504564
3502.580803	691561.606393	45.509569
3502.328186	691538.116340	45.514573
3502.298483	691507.972716	45.519578
3502.480869	691494.758908	45.524583
3502.313909	691457.075681	45.529588
3502.432018	691441.335110	45.534593
3502.152944	691405.361660	45.539597
3502.448154	691397.850457	45.544602
3502.536996	691363.109732	45.549607
3502.428343	691351.038194	45.554612
3502.371011	691319.654709	45.559617
3502.212292	691300.178410	45.564621
3501.811589	691265.965738	45.569626
3502.137301	691237.056175	45.574631
3502.210745	691236.745628	45.579636
3502.311472	691204.241155	45.584641
3502.287164	691188.125591	45.589645
3502.611257	691167.872916	45.594650
3502.553975	691139.026147	45.599655
3502.442994	691105.013880	45.604660
3502.564011	691074.744454	45.609665
3502.532536	691052.510252	45.614669
3502.400844	691020.491186	45.619674
3502.621442	690988.563213	45.624679
3502.078361	690975.468185	45.629684
3502.390527	690930.837846	45.634689
3502.251130	690928.124443	45.639693
3502.730374	690908.542164	45.644698
3502.701270	690886.307159	45.649703
3502.516973	690851.708966	45.654708
3502.727891	690814.856334	45.659713
3502.376020	690791.878216	45.664717
3502.574930	690775.177830	45.669722
3502.747619	690728.330523	45.674727
3502.163993	690718.873881	45.679732
3502.419408	690676.639850	45.684737
3502.353414	690672.421628	45.689741
3502.295842	690639.443642	45.694746
3502.462828	690615.931776	45.699751
3502.160289	690594.288410	45.704756
3502.608064	690561.326375	45.709761
3502.127844	690541.801891	45.714765
3502.363852	690516.238411	45.719770
3502.248041	690494.116231	45.724775
3502.330609	690481.613962	45.729780
3502.622685	690453.055706	45.734785
3502.538747	690432.271536	45.739789
3502.365443	690402.894196	45.744794
3502.665541	690363.487440	45.749799
3502.722659	690340.241740	45.754804
3502.908651	690315.034226	45.759809
3502.496791	690285.646056	45.764813
3502.409869	690228.240666	45.769818
3502.633247	690150.631906	45.774823
3502.372050	690006.923684	45.779828
3502.532658	689810.547859	45.784833
3502.315978	689553.023999	45.789837
3501.998842	689251.469391	45.794842
3501.869669	688883.238900	45.799847
3501.457805	688464.327401	45.804852
3501.520457	687980.468459	45.809857
3501.087442	687448.634724	45.814861
3500.720986	686849.262709	45.819866
3500.612148	686206.649789	45.824871
3499.454934	685503.926370	45.829876
3499.597390	684725.456615	45.834881
3498.760882	683924.077695	45.839885
3498.190341	683046.893650	45.844890
3497.491541	682104.804632	45.849895
3496.776673	681125.365609	45.854900
3496.439136	680062.672210	45.859905
3495.747277	678956.323064	45.864909
3495.104395	677789.495106	45.869914
3494.288111	676564.793828	45.874919
3493.021804	675276.261783	45.879924
3492.417314	673950.108175	45.884929
3491.396595	672561.818066	45.889933
3490.434159	671103.857147	45.894938
3489.595863	669595.282905	45.899943
3488.054035	668038.103839	45.904948
3487.305159	666410.100832	45.909953
3485.907843	664738.519188	45.914957
3484.596066	663007.896142	45.919962
3483.360283	661242.809747	45.924967
3481.805035	659420.543598	45.929972
3480.732930	657530.299578	45.934977
3479.038882	655601.787563	45.939981
3477.042995	653621.097760	45.944986
3475.932427	651599.946112	45.949991
3473.767069	649540.928775	45.954996
3472.704773	647429.774041	45.960001
3470.812329	645264.570711	45.965005
3468.996152	643057.338409	45.970010
3467.546680	640817.157681	45.975015
3465.751065	638518.864483	45.980020
3463.832938	636177.797948	45.985025
3461.576278	633807.931908	45.990029
3459.932890	631387.617792	45.995034
3458.264850	628923.789787	46.000039
3455.947679	626431.149056	46.005044
3453.881394	623881.277499	46.010049
3451.580731	621294.011487	46.015053
3449.642572	618686.321436	46.020058
3447.107973	616032.086789	46.025063
3445.052657	613346.596141	46.030068
3442.802604	610615.899608	46.035073
3440.441582	607864.187217	46.040077
3437.759569	605068.350675	46.045082
3435.738919	602239.444789	46.050087
3432.575418	599390.601387	46.055092
3430.244724	596499.189628	46.060097
3427.588280	593596.367746	46.065101
3425.207721	590643.749850	46.070106
3422.769444	587663.222000	46.075111
3419.566942	584661.924593	46.080116
3416.964926	581626.702549	46.085121
3414.057360	578576.949793	46.090125
3411.395489	575497.028134	46.095130
3408.372652	572393.916714	46.100135
3405.373531	569274.639611	46.105140
3402.949067	566122.288093	46.110145
3399.993558	562950.020128	46.115149
3396.639842	559755.944258	46.120154
3393.731611	556541.476042	46.125159
3390.171118	553305.581244	46.130164
3387.443859	550053.804958	46.135169
3384.151012	546794.139606	46.140173
3380.864083	543509.097323	46.145178
3378.365508	540192.235822	46.150183
3374.566206	536878.344553	46.155188
3371.965722	533531.346417	46.160193
3368.275320	530177.852139	46.165197
3365.078140	526799.027633	46.170202
3361.973671	523405.182693	46.175207
3358.406767	520004.237722	46.180212
3355.432243	516577.332346	46.185217
3351.715448	513151.915733	46.190221
3348.119961	509693.943873	46.195226
3344.780860	506249.487603	46.200231
3341.356494	502781.863545	46.205236
3337.754953	499313.942149	46.210241
3333.980947	495828.180732	46.215245
3330.232121	492337.802310	46.220250
3326.997136	488835.953570	46.225255
3323.444105	485333.404917	46.230260
3319.896630	481814.875752	46.235265
3316.470347	478295.539112	46.240269
3312.480572	474763.769284	46.245274
3309.096979	471231.129212	46.250279
3305.319385	467690.397917	46.255284
3301.733893	464136.925171	46.260289
3297.948837	460589.481405	46.265293
3294.137949	457021.491067	46.270298
3290.447116	453452.449872	46.275303
3286.680635	449894.013153	46.280308
3282.807078	446315.266261	46.285313
3279.018207	442754.830934	46.290317
3275.190032	439180.583736	46.295322
3271.480988	435609.755206	46.300327
3267.770698	432042.073858	46.305332
3263.704505	428451.827075	46.310337
3259.826975	424884.613635	46.315341
3255.974179	421305.145751	46.320346
3252.281332	417730.925787	46.325351
3248.457402	414160.923577	46.330356
3244.682538	410584.964199	46.335361
3240.896290	407012.693034	46.340365
3236.915689	403431.070779	46.345370
3233.041782	399858.474903	46.350375
3228.975900	396281.096177	46.355380
3225.023127	392705.628145	46.360385
3220.796479	389136.136857	46.365389
3217.292339	385582.511485	46.370394
3213.549934	382017.371076	46.375399
3209.198273	378464.300839	46.380404
3205.626880	374899.415094	46.385409
3201.551536	371352.862537	46.390413
3197.506460	367811.245811	46.395418
3193.619010	364267.384164	46.400423
3189.890022	360728.943980	46.405428
3186.034631	357181.383344	46.410433
3181.581642	353648.956579	46.415437
3177.815995	350125.920140	46.420442
3173.910929	346599.014444	46.425447
3169.524127	343090.214785	46.430452
3165.764635	339581.208742	46.435457
3161.964712	336074.000299	46.440461
3157.844455	332570.097310	46.445466
3154.291651	329063.943185	46.450471
3149.861889	325566.986140	46.455476
3145.764909	322083.773562	46.460481
3141.802164	318592.483344	46.465485
3137.813771	315136.939196	46.470490
3133.843363	311671.373326	46.475495
3129.699088	308222.814345	46.480500
3125.822439	304773.174941	46.485505
3122.065897	301329.160554	46.490509
3117.783477	297901.735768	46.495514
3113.822740	294474.780869	46.500519
3109.638660	291058.632547	46.505524
3105.906628	287657.086354	46.510529
3101.973239	284248.003359	46.515533
3098.011181	280849.623882	46.520538
3094.009907	277454.014164	46.525543
3089.817571	274083.645839	46.530548
3085.569076	270701.069443	46.535553
3081.584376	267345.207332	46.540557
3077.727426	263990.649176	46.545562
3073.733430	260647.507860	46.550567
3069.511296	257313.108015	46.555572
3065.947192	253988.433178	46.560577
3062.076769	250673.982390	46.565581
3058.038023	247347.278955	46.570586
3054.048744	244038.475392	46.575591
3049.790364	240750.433955	46.580596
3045.812771	237454.778098	46.585601
3041.730526	234181.529055	46.590605
3037.934087	230913.669482	46.595610
3033.973710	227648.098586	46.600615
3029.920617	224401.492357	46.605620
3025.854825	221155.561382	46.610625
3021.793068	217917.313593	46.615629
3017.995652	214695.931037	46.620634
3014.026847	211487.672868	46.625639
3009.659115	208285.136124	46.630644
3005.923417	205043.769629	46.635649
3002.135375	201808.493289	46.640653
2997.900229	198641.406130	46.645658
2994.030581	195464.821059	46.650663
2989.948135	192308.064670	46.655668
2986.186683	189158.148824	46.660673
2982.089366	186017.186448	46.665677
2977.993768	182891.147080	46.670682
2974.235620	179758.832161	46.675687
2970.102863	176651.146544	46.680692
2966.066925	173541.398964	46.685697
2962.441076	170445.778951	46.690701
2958.313817	167375.648803	46.695706
2954.590875	164290.003305	46.700711
2950.336632	161228.221327	46.705716
2946.587429	158171.043410	46.710721
2942.345913	155125.507561	46.715725
2938.404149	152092.008860	46.720730
2934.221051	149058.332003	46.725735
2930.174204	146056.729196	46.730740
2926.662912	143044.225572	46.735745
2922.597267	140046.625772	46.740749
2918.515828	137078.766806	46.745754
2914.465852	134093.091126	46.750759
2910.060897	131141.729625	46.755764
2906.412526	128195.077531	46.760769
2902.369358	125258.094749	46.765773
2898.500619	122336.039888	46.770778
2894.798235	119405.057951	46.775783
2890.557116	116514.103642	46.780788
2886.599767	113602.512738	46.785793
2882.575336	110728.509637	46.790797
2878.443540	107858.760825	46.795802
2874.570647	104990.899524	46.800807
2870.196216	102151.178686	46.805812
2866.290561	99317.745972	46.810817
2862.310895	96496.019377	46.815821
2858.277078	93680.926970	46.820826
2854.433680	90884.367084	46.825831
2849.909235	88101.083494	46.830836
2846.024700	85335.724771	46.835841
2841.694167	82589.204864	46.840845
2837.417335	79853.848291	46.845850
2833.431637	77128.259985	46.850855
2829.320063	74428.038623	46.855860
2825.278930	71731.446090	46.860865
2820.886652	69061.731345	46.865869
2816.690672	66408.074501	46.870874
2812.705021	63772.892899	46.875879
2807.757249	61159.951566	46.880884
2803.781189	58550.407746	46.885889
2799.468563	55988.091241	46.890893
2794.861097	53433.683502	46.895898
2790.643106	50893.969992	46.900903
2785.811434	48403.770079	46.905908
2780.758166	45929.733341	46.910913
2775.375786	43501.054780	46.915917
2768.331511	41155.301458	46.920922
2760.222552	38881.026832	46.925927
2751.856573	36696.519298	46.930932
2743.485989	34604.618609	46.935937
2735.411320	32596.539157	46.940941
2727.627974	30670.721439	46.945946
2720.521976	28850.166401	46.950951
2713.085222	27125.201954	46.955956
2706.287174	25478.710004	46.960961
2699.328526	23933.441561	46.965965
2692.687485	22476.378701	46.970970
2687.150376	21082.085585	46.975975
2680.741631	19777.094708	46.980980
2674.711636	18541.162291	46.985985
2669.630881	17373.733767	46.990989
2664.203676	16281.889675	46.995994
2658.793343	15230.470052	47.000999
2653.308832	14249.324620	47.006004
2647.730081	13344.609683	47.011009
2642.171827	12489.499508	47.016013
2636.350192	11688.000390	47.021018
2631.488382	10953.015032	47.026023
2625.762990	10266.633725	47.031028
2620.621912	9630.146098	47.036033
2615.765666	9035.987532	47.041037
2610.966094	8482.005732	47.046042
2606.660681	7976.122224	47.051047
2602.119508	7506.829686	47.056052
2598.135589	7060.422112	47.061057
2593.983208	6639.744162	47.066061
2589.923875	6247.180475	47.071066
2586.697661	5870.336469	47.076071
2582.732130	5526.976695	47.081076
2579.251570	5190.564805	47.086081
2575.494227	4854.805851	47.091085
2571.981076	4546.197506	47.096090
2568.921463	4244.106141	47.101095
2565.738103	3964.490387	47.106100
2562.599035	3664.458736	47.111105
2559.509814	3379.445300	47.116109
2556.044936	3094.728397	47.121114
2552.549637	2816.740704	47.126119
2549.469005	2551.084005	47.131124
2546.479259	2261.754441	47.136129
2543.258601	2000.387825	47.141133
2539.887751	1731.898821	47.146138
2536.557043	1455.850622	47.151143
2533.052884	1202.344931	47.156148
2529.610281	946.524611	47.161153
2525.853189	685.062998	47.166157
2521.898241	446.857570	47.171162
2517.702981	211.494566	47.176167
2508.632252	134.518266	47.181172
2496.246182	187.964077	47.186177
2490.270644	184.708430	47.191181
2486.777955	191.562421	47.196186
2484.409817	181.998712	47.201191
2483.203702	183.107999	47.206196
2481.566367	176.662623	47.211201
2479.499385	180.140209	47.216205
2476.093679	179.860776	47.221210
2473.168278	176.190291	47.226215
2469.248297	187.300420	47.231220
2466.083201	184.852759	47.236225
2463.033475	177.799856	47.241229
2459.634123	189.564872	47.246234
2456.361351	181.447825	47.251239
2453.043680	190.006782	47.256244
2449.762746	184.709904	47.261249
2446.638936	181.195918	47.266253
2443.155910	185.482909	47.271258
2440.189931	172.869544	47.276263
2436.125889	178.280197	47.281268
2432.637083	174.933827	47.286273
2429.570378	168.993401	47.291277
2426.568032	182.893637	47.296282
2422.984592	170.935359	47.301287
2419.262980	178.430447	47.306292
2416.004043	174.871694	47.311297
2412.934282	177.697653	47.316301
2409.388993	174.655845	47.321306
2405.776771	170.036893	47.326311
2402.351038	177.090638	47.331316
2399.634519	171.253651	47.336321
2395.909334	174.981521	47.341325
2391.703274	169.141587	47.346330
2388.957591	169.829750	47.351335
2385.628034	163.533529	47.356340
2381.835457	169.219493	47.361345
2378.485486	169.106758	47.366349
2374.847882	169.107420	47.371354
2371.689731	157.240413	47.376359
2368.246765	177.579413	47.381364
2365.178280	170.016001	47.386369
2361.777423	173.367898	47.391373
2357.552573	169.142186	47.396378
2354.658877	170.904654	47.401383
2351.131699	166.373139	47.406388
2347.561037	164.193211	47.411393
2344.046036	172.988456	47.416397
2340.453678	170.530706	47.421402
2337.206258	158.146827	47.426407
2333.521275	165.814118	47.431412
2330.180643	159.977993	47.436417
2326.692044	155.246738	47.441421
2323.160783	167.653635	47.446426
2319.922232	162.766644	47.451431
2316.539662	168.872000	47.456436
2312.797321	168.868489	47.461441
2309.178800	165.192561	47.466445
2305.875729	171.011680	47.471450
2302.420340	167.718699	47.476455
2299.211991	167.471533	47.481460
2295.131168	168.273616	47.486465
2292.131466	163.114546	47.491469
2288.895529	163.739253	47.496474
2285.501812	159.416644	47.501479
2281.885231	157.321310	47.506484
2278.295224	157.152762	47.511489
2274.825894	156.653679	47.516493
2270.839261	164.289709	47.521498
2267.730063	156.491353	47.526503
2264.055743	157.189246	47.531508
2260.451865	163.744996	47.536513
2257.205276	159.488104	47.541517
2253.666287	165.272598	47.546522
2250.598889	155.181169	47.551527
2247.148293	166.804573	47.556532
2243.438724	158.650493	47.561537
2239.773223	153.745648	47.566541
2236.000028	164.380367	47.571546
2233.004971	163.897334	47.576551
2229.557430	155.847218	47.581556
2225.949835	163.296964	47.586561
2222.463744	159.323949	47.591565
2218.889942	167.312582	47.596570
2215.389368	159.919100	47.601575
2211.910772	167.904845	47.606580
2208.293985	162.573618	47.611585
2205.374426	155.074146	47.616589
2201.652174	165.129572	47.621594
2198.512875	155.014928	47.626599
2194.902874	161.637250	47.631604
2191.234170	170.228067	47.636609
2187.756617	164.816439	47.641613
2183.909469	162.378188	47.646618
2180.508469	158.672166	47.651623
2176.925140	159.865617	47.656628
2173.044069	155.902014	47.661633
2170.240374	152.721755	47.666637
2166.904803	161.792958	47.671642
2163.405094	160.511980	47.676647
2159.887469	159.017480	47.681652
2156.243068	156.049661	47.686657
2152.624637	157.635120	47.691661
2149.021578	163.937820	47.696666
2145.623464	153.670786	47.701671
2141.957172	156.475427	47.706676
2138.741180	150.184522	47.711681
2135.638881	152.777236	47.716685
2131.993895	162.454079	47.721690
2128.427917	151.263405	47.726695
2124.621546	163.008581	47.731700
2121.216256	159.476773	47.736705
2117.936180	158.484578	47.741709
2113.923931	155.945181	47.746714
2110.711209	157.118723	47.751719
2107.415543	157.753018	47.756724
2103.820277	154.704702	47.761729
2100.743141	145.562230	47.766733
2096.950104	153.805595	47.771738
2093.470439	147.148591	47.776743
2089.710690	162.905898	47.781748
2086.130643	153.647960	47.786753
2082.683710	145.442364	47.791757
2078.739400	160.320419	47.796762
2075.751321	151.675745	47.801767
2072.568554	159.593972	47.806772
2069.376518	142.430094	47.811777
2065.709265	140.761262	47.816781
2061.652757	151.456494	47.821786
2058.613861	146.828391	47.826791
2054.789104	155.289166	47.831796
2051.315392	154.550806	47.836801
2048.155112	141.316259	47.841805
2044.263186	154.720238	47.846810
2041.025568	147.307748	47.851815
2037.484761	144.598205	47.856820
2033.640185	148.386504	47.861825
2030.140948	143.925620	47.866829
2026.893948	151.061569	47.871834
2023.455916	136.939305	47.876839
2019.726361	144.529502	47.881844
2016.272256	153.789881	47.886849
2013.315771	144.907375	47.891853
2009.590744	146.470878	47.896858
2006.571947	142.665358	47.901863
2002.608609	146.152027	47.906868
1998.688663	150.101399	47.911873
1995.444941	146.378028	47.916877
1991.621701	145.644751	47.921882
1988.460667	144.553655	47.926887
1984.808986	141.634341	47.931892
1981.312146	142.698206	47.936897
1978.170008	139.847479	47.941901
1974.046244	150.731291	47.946906
1970.799665	145.184994	47.951911
1967.256899	145.175825	47.956916
1963.854667	146.925420	47.961921
1960.738745	144.409798	47.966925
1957.244113	146.816801	47.971930
1953.972199	140.780565	47.976935
1950.367890	144.552529	47.981940
1946.686794	146.000879	47.986945
1943.328973	138.976161	47.991949
1939.221235	148.807704	47.996954
1935.565234	147.750248	48.001959
1932.441736	145.542561	48.006964
1928.693912	150.531359	48.011969
1925.810792	145.216531	48.016973
1921.850832	144.915176	48.021978
1918.709344	137.402443	48.026983
1914.991808	146.030508	48.031988
1911.375396	147.384134	48.036993
1908.270269	143.243256	48.041997
1904.305583	140.112261	48.047002
1900.847654	138.238481	48.052007
1897.535284	144.740596	48.057012
1893.910637	147.136362	48.062017
1890.598491	142.606400	48.067021
1886.779711	147.821456	48.072026
1883.445681	150.629814	48.077031
1879.883563	144.819768	48.082036
1876.351917	143.014228	48.087041
1873.132403	140.069003	48.092045
1869.520921	146.512009	48.097050
1865.655800	133.103368	48.102055
1862.289302	143.613321	48.107060
1859.243443	140.778742	48.112065
1855.593511	136.723952	48.117069
1852.090091	148.852611	48.122074
1848.625869	135.957343	48.127079
1845.121127	136.190630	48.132084
1841.397703	136.115886	48.137089
1838.182908	143.298526	48.142093
1834.355716	140.692493	48.147098
1831.096491	149.147816	48.152103
1827.283520	142.192654	48.157108
1823.804131	148.884818	48.162113
1820.815328	131.943736	48.167117
1816.966153	134.933934	48.172122
1813.647566	138.777394	48.177127
1809.934201	141.532629	48.182132
1806.417100	140.293273	48.187137
1802.982094	140.747141	48.192141
1799.436956	145.438904	48.197146
1796.086009	141.889487	48.202151
1792.788815	147.120865	48.207156
1788.922612	142.050632	48.212161
1785.664358	138.126557	48.217165
1781.890588	137.274375	48.222170
1778.366104	146.195658	48.227175
1775.039679	147.681451	48.232180
1771.495019	141.722185	48.237185
1768.192157	139.574239	48.242189
1764.212756	158.759103	48.247194
1761.149364	140.233121	48.252199
1757.338723	141.920287	48.257204
1753.830305	143.202711	48.262209
1750.406243	141.495528	48.267213
1747.000744	137.742234	48.272218
1743.407990	138.154520	48.277223
1740.127831	137.126097	48.282228
1736.688456	143.857291	48.287233
1733.453565	132.601617	48.292237
1729.261387	143.520789	48.297242
1726.134298	133.268341	48.302247
1722.050529	139.524057	48.307252
1718.699412	141.315699	48.312257
1715.637305	132.219189	48.317261
1711.937487	137.505692	48.322266
1708.264899	139.446757	48.327271
1704.885704	137.551434	48.332276
1701.287026	137.139264	48.337281
1698.268329	132.963535	48.342285
1694.302740	132.650474	48.347290
1691.044145	127.369234	48.352295
1687.680898	133.516780	48.357300
1683.965650	133.292214	48.362305
1680.697485	133.433845	48.367309
1676.803627	136.535731	48.372314
1673.431872	131.630185	48.377319
1670.069340	131.478187	48.382324
1666.138480	136.097610	48.387329
1662.910643	122.060928	48.392333
1658.891684	132.393059	48.397338
1655.866316	124.445748	48.402343
1652.736308	130.928339	48.407348
1648.853552	131.138391	48.412353
1645.319677	129.365762	48.417357
1641.665059	127.664001	48.422362
1638.447673	126.636330	48.427367
1634.998139	132.746465	48.432372
1631.858774	124.594227	48.437377
1628.542447	122.753301	48.442381
1624.455207	129.302713	48.447386
1621.057612	129.010514	48.452391
1617.409007	132.504092	48.457396
1613.710521	136.207990	48.462401
1610.081666	122.740041	48.467405
1606.436202	134.144992	48.472410
1603.550975	127.211771	48.477415
1599.977149	128.520902	48.482420
1596.283691	126.958009	48.487425
1592.960654	118.063970	48.492429
1589.709326	122.683249	48.497434
1586.066400	120.740822	48.502439
1582.836172	124.334604	48.507444
1578.839855	131.253049	48.512449
1575.222815	117.628668	48.517453
1571.750222	121.712834	48.522458
1568.364025	122.815154	48.527463
1564.760765	118.740069	48.532468
1561.183630	128.960580	48.537473
1558.118738	128.143781	48.542477
1554.321483	128.689860	48.547482
1550.776289	129.116339	48.552487
1547.307289	115.607040	48.557492
1543.693907	122.383488	48.562497
1540.280373	116.487806	48.567501
1536.691355	123.518746	48.572506
1533.935302	117.204199	48.577511
1529.980543	114.973535	48.582516
1526.343211	123.943419	48.587521
1522.927728	117.425866	48.592525
1519.286502	126.788116	48.597530
1515.763537	120.078559	48.602535
1512.313153	120.886837	48.607540
1508.698336	126.663046	48.612545
1505.455065	114.266566	48.617549
1501.702326	125.896317	48.622554
1498.492212	122.604273	48.627559
1495.006637	116.832226	48.632564
1491.245142	127.107523	48.637569
1487.753178	114.144359	48.642573
1483.955061	121.473734	48.647578
1480.782550	123.165968	48.652583
1477.280197	124.275908	48.657588
1473.549362	122.818160	48.662593
1470.399048	124.594942	48.667597
1466.523153	130.791050	48.672602
1463.418907	123.581148	48.677607
1459.791620	125.638646	48.682612
1456.297704	130.251338	48.687617
1452.883673	123.377995	48.692621
1449.423944	124.128861	48.697626
1446.115375	127.611556	48.702631
1442.510602	124.158040	48.707636
1438.555632	128.135543	48.712641
1435.592144	126.620659	48.717645
1431.424031	134.763878	48.722650
1428.138191	127.064622	48.727655
1424.960874	123.103958	48.732660
1420.860797	132.768071	48.737665
1417.878475	126.237811	48.742669
1413.901285	133.727478	48.747674
1410.812506	129.667728	48.752679
1407.351939	125.137213	48.757684
1403.991369	121.910363	48.762689
1400.662235	126.038823	48.767693
1396.637820	130.308651	48.772698
1393.019092	125.698319	48.777703
1389.822815	124.220956	48.782708
1386.119071	119.207512	48.787713
1383.018729	119.619396	48.792717
1379.167426	123.526728	48.797722
1375.502128	119.463237	48.802727
1372.096433	127.809046	48.807732
1368.361543	126.650232	48.812737
1365.280586	121.022362	48.817741
1362.129593	124.073144	48.822746
1358.258126	115.565366	48.827751
1354.751344	124.653505	48.832756
1351.041634	125.102595	48.837761
1347.666296	123.258606	48.842765
1344.216132	124.815672	48.847770
1340.560773	118.366334	48.852775
1337.010531	120.634971	48.857780
1333.550236	124.809233	48.862785
1330.781892	123.383523	48.867789
1326.764796	123.921925	48.872794
1323.540205	131.543400	48.877799
1319.632210	124.897652	48.882804
1316.009949	130.645237	48.887809
1312.942220	119.619021	48.892813
1309.125043	127.626968	48.897818
1305.839738	115.501050	48.902823
1301.917879	119.819517	48.907828
1298.556171	117.397878	48.912833
1295.555842	115.144229	48.917837
1291.761519	108.726395	48.922842
1288.027735	110.838334	48.927847
1284.673614	123.637077	48.932852
1281.165672	119.186723	48.937857
1277.701916	115.746540	48.942861
1274.085238	122.767437	48.947866
1270.777603	119.209687	48.952871
1266.939669	115.679618	48.957876
1263.478629	123.026054	48.962881
1260.215520	114.353465	48.967885
1256.533687	126.227018	48.972890
1253.081666	117.314522	48.977895
1249.859363	114.540912	48.982900
1246.186979	114.511096	48.987905
1242.810013	108.306106	48.992909
1238.905632	117.279487	48.997914
1235.728793	117.947039	49.002919
1232.100955	114.835748	49.007924
1228.368248	117.922009	49.012929
1224.983683	128.245886	49.017933
1221.401664	122.262279	49.022938
1218.045090	124.972203	49.027943
1214.572259	115.086164	49.032948
1210.900399	115.038529	49.037953
1207.846279	105.918408	49.042957
1203.897601	110.433002	49.047962
1200.703672	117.500880	49.052967
1197.429794	109.986323	49.057972
1193.270498	115.625050	49.062977
1190.076487	111.762440	49.067981
1186.314975	122.332578	49.072986
1183.349033	108.397074	49.077991
1179.908670	112.525325	49.082996
1175.848327	115.417546	49.088001
1172.719699	107.400454	49.093005
1169.152289	120.850023	49.098010
1165.584022	112.619878	49.103015
1161.729653	116.742198	49.108020
1157.981500	110.951290	49.113025
1154.925921	108.552950	49.118029
1151.483470	111.364342	49.123034
1148.328783	105.193917	49.128039
1144.709452	105.155411	49.133044
1141.247125	107.657909	49.138049
1137.937632	102.037612	49.143053
1134.012273	109.511027	49.148058
1130.540509	117.537967	49.153063
1127.280908	103.536218	49.158068
1123.098903	107.375887	49.163073
1120.054472	109.982761	49.168077
1116.196764	118.241461	49.173082
1113.125042	108.176512	49.178087
1109.431739	108.963886	49.183092
1105.601242	105.290255	49.188097
1102.991524	101.815560	49.193101
1099.237978	112.905408	49.198106
1095.285501	110.252453	49.203111
1091.774629	105.027012	49.208116
1088.240275	107.827992	49.213121
1085.026261	113.809963	49.218125
1081.464515	118.196938	49.223130
1078.139472	117.642528	49.228135
1074.690683	114.135899	49.233140
1070.960333	116.710199	49.238145
1067.732138	111.529399	49.243149
1063.914805	108.165026	49.248154
1060.231339	119.791914	49.253159
1056.977764	109.951654	49.258164
1053.248607	115.863725	49.263169
1050.097308	105.032901	49.268173
1045.978695	120.473659	49.273178
1042.742294	111.293228	49.278183
1039.576656	118.049474	49.283188
1036.165272	114.064857	49.288193
1032.792489	107.234184	49.293197
1029.006707	114.833395	49.298202
1025.547104	109.869881	49.303207
1022.312368	112.234781	49.308212
1018.119520	104.818470	49.313217
1014.605127	105.716641	49.318221
1011.169391	101.824482	49.323226
1008.170410	111.122903	49.328231
1004.517367	101.872091	49.333236
1000.653886	111.665927	49.338241
997.471451	99.122680	49.343245
993.982429	108.165295	49.348250
990.505016	105.668505	49.353255
986.940876	102.251673	49.358260
983.292708	109.984449	49.363265
980.032900	99.035273	49.368269
976.312086	111.872735	49.373274
972.744774	109.276175	49.378279
969.081338	108.043916	49.383284
965.758551	109.354050	49.388289
962.677960	100.290005	49.393293
958.916801	100.970520	49.398298
955.146245	105.325223	49.403303
951.788046	104.769683	49.408308
948.572162	106.401172	49.413313
945.388077	94.488540	49.418317
941.705822	101.420072	49.423322
937.989329	107.321846	49.428327
934.030691	99.450705	49.433332
930.499438	105.769407	49.438337
927.466856	99.043388	49.443341
923.458168	96.351543	49.448346
920.325616	97.815150	49.453351
916.764601	101.768772	49.458356
913.491296	102.371005	49.463361
910.154601	104.971889	49.468365
906.163724	101.271880	49.473370
902.224137	100.957383	49.478375
899.417573	105.270893	49.483380
895.925442	107.656747	49.488385
892.871157	94.236943	49.493389
888.632432	105.732198	49.498394
885.033457	108.339976	49.503399
882.128313	103.578708	49.508404
878.471962	106.827457	49.513409
874.862826	110.126416	49.518413
871.208584	109.767117	49.523418
867.761927	104.646882	49.528423
864.272162	98.615773	49.533428
860.797851	104.606211	49.538433
857.111235	96.568001	49.543437
853.704535	107.927835	49.548442
850.311840	100.417629	49.553447
847.005993	100.646012	49.558452
843.442633	105.097366	49.563457
839.682336	98.448372	49.568461
836.291885	108.181649	49.573466
832.786850	95.563244	49.578471
829.238837	104.655590	49.583476
825.398179	100.282757	49.588481
821.977896	94.938960	49.593485
818.879827	88.634320	49.598490
815.572268	99.257102	49.603495
811.728177	94.277055	49.608500
808.179965	97.892775	49.613505
804.694227	90.764063	49.618509
801.081876	91.755171	49.623514
797.605344	101.395161	49.628519
794.295674	89.814436	49.633524
790.711256	99.375384	49.638529
787.376702	85.723795	49.643533
783.912420	90.698713	49.648538
780.245590	90.283950	49.653543
776.477169	92.057877	49.658548
772.825866	101.098872	49.663553
769.503879	87.702150	49.668557
766.110538	84.441367	49.673562
763.101637	87.224341	49.678567
759.610657	92.286377	49.683572
755.483371	94.842135	49.688577
751.939208	89.710506	49.693581
748.201715	93.372187	49.698586
745.208669	93.783531	49.703591
742.094959	85.630330	49.708596
738.342696	90.002898	49.713601
735.187873	91.849005	49.718605
731.010807	92.224960	49.723610
727.286370	89.941923	49.728615
724.004191	86.386316	49.733620
720.627954	88.393976	49.738625
717.455202	83.549034	49.743629
713.497172	94.804206	49.748634
710.024533	92.508140	49.753639
706.653923	88.323664	49.758644
703.039549	96.084203	49.763649
699.806594	87.309421	49.768653
696.100970	97.962219	49.773658
692.937993	90.853416	49.778663
689.324139	86.703081	49.783668
684.990454	97.254567	49.788673
682.149977	87.775497	49.793677
678.508989	100.529899	49.798682
674.826809	95.594429	49.803687
671.777628	91.036524	49.808692
668.543198	94.200042	49.813697
664.896756	97.356939	49.818701
661.061660	93.067996	49.823706
657.321902	93.158742	49.828711
653.990729	86.907006	49.833716
650.490134	100.210670	49.838721
647.202740	79.795617	49.843725
643.419605	98.580458	49.848730
639.942088	98.731431	49.853735
636.556957	93.738560	49.858740
632.954023	98.550049	49.863745
629.572898	91.061999	49.868749
626.118822	96.532040	49.873754
623.008692	89.864870	49.878759
619.202743	96.216224	49.883764
615.274641	93.240984	49.888769
611.997433	94.005900	49.893773
608.244086	93.186653	49.898778
604.804481	86.511854	49.903783
601.618920	93.363627	49.908788
597.816956	94.705563	49.913793
595.064183	99.780356	49.918797
590.875156	107.004199	49.923802
587.291809	100.405685	49.928807
583.909429	99.531785	49.933812
580.319824	102.794196	49.938817
577.338910	91.749690	49.943821
573.855861	95.707249	49.948826
570.220807	96.477734	49.953831
566.536308	84.257117	49.958836
562.871077	92.984041	49.963841
559.305350	94.073797	49.968845
555.548965	92.367286	49.973850
552.444467	93.028679	49.978855
549.283878	93.153328	49.983860
545.255759	96.787095	49.988865
541.677285	85.515113	49.993869
538.703948	91.729737	49.998874
535.124327	95.706463	50.003879
531.784809	88.495185	50.008884
528.082863	95.774638	50.013889
524.618629	96.284037	50.018893
520.937455	92.036058	50.023898
517.287285	86.452714	50.028903
513.842422	89.354765	50.033908
510.119723	94.358047	50.038913
506.557054	96.781723	50.043917
503.232561	96.330275	50.048922
500.020436	96.084407	50.053927
496.837123	101.154729	50.058932
492.948842	106.462884	50.063937
489.681769	99.214191	50.068941
486.075666	102.380146	50.073946
482.478373	96.476881	50.078951
478.999391	93.150977	50.083956
475.304244	106.256075	50.088961
472.235581	104.634144	50.093965
468.160424	95.559268	50.098970
464.506286	89.983337	50.103975
461.450213	89.766136	50.108980
457.659775	95.120877	50.113985
454.810638	97.351716	50.118989
451.274584	88.091736	50.123994
447.335741	104.267269	50.128999
443.994683	90.102020	50.134004
440.205720	103.573135	50.139009
436.862634	94.131845	50.144013
433.401682	94.356610	50.149018
429.847988	98.391486	50.154023
426.339983	92.103097	50.159028
422.606200	95.284314	50.164033
419.076046	88.017461	50.169037
415.698727	96.624819	50.174042
412.436793	101.745310	50.179047
409.478694	88.070238	50.184052
405.562160	100.557659	50.189057
401.849563	91.539472	50.194061
397.973591	98.729628	50.199066
394.324142	98.070973	50.204071
391.296725	92.834789	50.209076
387.604215	93.889034	50.214081
384.752455	99.603320	50.219085
380.993020	102.494592	50.224090
377.415611	101.012782	50.229095
374.010895	95.030577	50.234100
370.079647	98.837712	50.239105
366.870501	89.661242	50.244109
363.000154	94.004525	50.249114
359.808821	94.870462	50.254119
356.751809	94.240271	50.259124
352.737104	99.712339	50.264129
349.279165	87.360107	50.269133
345.496839	92.801214	50.274138
342.454139	93.928894	50.279143
339.146803	91.641293	50.284148
335.555281	103.413506	50.289153
331.866404	83.962299	50.294157
328.113795	84.504196	50.299162
324.697463	89.435405	50.304167
321.289304	86.568951	50.309172
317.523339	88.805216	50.314177
314.279833	85.628929	50.319181
310.937115	83.821404	50.324186
306.847151	100.722789	50.329191
303.617735	80.985596	50.334196
300.235941	93.074760	50.339201
296.709877	88.379406	50.344205
293.199519	91.850730	50.349210
289.845288	93.382062	50.354215
286.453959	89.274178	50.359220
282.855845	94.292935	50.364225
279.534433	80.657795	50.369229
275.383211	90.667747	50.374234
272.083276	90.167816	50.379239
268.608216	92.936921	50.384244
265.205358	92.529809	50.389249
261.661532	95.191903	50.394253
258.546365	92.815524	50.399258
254.884243	91.035462	50.404263
251.446605	88.525201	50.409268
247.459893	97.557582	50.414273
244.206925	88.801296	50.419277
240.185385	92.610073	50.424282
237.195497	91.276605	50.429287
233.875685	90.962924	50.434292
230.057385	95.071560	50.439297
226.394950	85.247614	50.444301
222.911773	100.278713	50.449306
219.682050	101.493683	50.454311
216.494255	84.873689	50.459316
212.780738	103.447203	50.464321
209.570845	95.866046	50.469325
205.840749	96.266780	50.474330
201.930057	99.718614	50.479335
198.520948	91.910954	50.484340
194.848597	101.336524	50.489345
191.572979	93.380672	50.494349
188.089523	94.867764	50.499354
184.345281	94.857640	50.504359
181.198004	95.593475	50.509364
177.476338	98.558981	50.514369
174.091599	93.919268	50.519373
170.667411	97.003854	50.524378
167.299743	103.815030	50.529383
163.996421	97.047204	50.534388
160.139360	100.186103	50.539393
156.678285	91.925715	50.544397
153.144474	99.132042	50.549402
149.275148	102.830847	50.554407
146.337449	98.886351	50.559412
142.622555	91.780574	50.564417
139.300930	95.237939	50.569421
135.621748	89.752494	50.574426
131.598784	88.869775	50.579431
128.688476	95.700167	50.584436
125.169439	99.789732	50.589441
121.495810	90.829301	50.594445
117.949514	82.874922	50.599450
114.693007	96.974830	50.604455
111.131027	92.210005	50.609460
107.509500	92.394331	50.614465
104.317035	96.268024	50.619469
100.675056	92.322567	50.624474
96.808065	99.244097	50.629479
93.506690	95.917527	50.634484
89.923713	96.777670	50.639489
86.520156	86.193879	50.644493
82.872295	90.458530	50.649498
79.256067	89.279802	50.654503
76.022095	97.052813	50.659508
72.330116	101.199671	50.664513
69.029325	90.833310	50.669517
65.876445	97.529661	50.674522
62.410210	90.243074	50.679527
58.927647	94.056106	50.684532
55.060036	91.525448	50.689537
51.622730	87.098590	50.694541
47.874146	92.135149	50.699546
44.322264	92.414950	50.704551
41.284261	88.785909	50.709556
37.093824	95.527800	50.714561
33.990996	89.618445	50.719565
30.365023	84.644659	50.724570
26.840178	87.666301	50.729575
23.585779	84.427719	50.734580
19.688068	101.554027	50.739585
16.778915	82.042318	50.744589
12.984125	89.212440	50.749594
9.399662	97.775057	50.754599
6.123742	88.337435	50.759604
2.123549	98.666968	50.764609