Tue Jun 21 10:46:32 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.161551	85.684978	0.000000
-0.125923	100.082077	0.005005
-0.120579	87.665028	0.010010
-0.259063	96.253186	0.015014
-0.270060	85.580323	0.020019
-0.526789	75.772225	0.025024
-0.769494	76.364679	0.030029
-0.891596	66.205535	0.035034
-1.026945	60.134985	0.040038
-1.472456	64.327440	0.045043
-1.538838	46.464831	0.050048
-2.084273	39.028961	0.055053
-1.989910	32.388568	0.060058
-2.553344	25.693713	0.065062
-2.560263	9.480679	0.070067
-2.688953	6.429038	0.075072
-3.495710	6.872172	0.080077
-3.589948	-0.110330	0.085082
-3.977091	-3.790103	0.090086
-4.544070	-2.864531	0.095091
-4.988069	-8.622476	0.100096
-5.696219	2.580303	0.105101
-5.214803	-2.015267	0.110106
-5.390655	1.183937	0.115110
-5.812206	8.408186	0.120115
-5.534413	3.540663	0.125120
-6.072277	5.430322	0.130125
-6.217145	3.880107	0.135130
-6.547795	3.478946	0.140134
-7.537140	3.455629	0.145139
-7.198352	2.384764	0.150144
-7.796800	-1.417491	0.155149
-7.293288	-4.660053	0.160154
-7.233596	-4.804003	0.165158
-7.794932	4.209327	0.170163
-8.460729	5.280715	0.175168
-8.743852	-2.554561	0.180173
-9.037390	-2.921414	0.185178
-8.904745	-3.000484	0.190182
-9.563843	0.712481	0.195187
-10.198272	-6.417562	0.200192
-10.519429	2.783717	0.205197
-10.262588	3.119003	0.210202
-10.657209	-6.787763	0.215206
-10.744147	-0.529227	0.220211
-10.390711	-6.864013	0.225216
-10.438515	11.381568	0.230221
-11.293892	-1.718124	0.235226
-11.590679	-0.989437	0.240230
-12.116960	6.713518	0.245235
-12.130001	-1.181084	0.250240
-11.908826	6.202144	0.255245
-12.739136	7.876594	0.260250
-13.158361	0.096613	0.265254
-13.733559	-2.781629	0.270259
-13.496116	-2.468982	0.275264
-13.526897	-0.426889	0.280269
-13.650232	-8.062872	0.285274
-14.019703	-10.354567	0.290278
-14.722256	-7.575292	0.295283
-14.981039	-7.522844	0.300288
-15.148687	-4.913448	0.305293
-15.293531	-3.930696	0.310298
-15.480983	-8.391625	0.315302
-15.577631	-6.276466	0.320307
-15.542871	-7.645672	0.325312
-16.323679	6.951828	0.330317
-16.933727	0.318579	0.335322
-16.976672	-5.417769	0.340326
-16.942913	-0.156216	0.345331
-17.021695	-6.251498	0.350336
-17.351321	8.129999	0.355341
-17.284165	-3.648773	0.360346
-17.781805	9.272063	0.365350
-18.473075	6.804550	0.370355
-18.430165	-10.428638	0.375360
-18.609498	3.179482	0.380365
-18.595896	1.264205	0.385370
-19.103663	-4.026945	0.390374
-19.596404	12.664515	0.395379
-19.766167	-8.363106	0.400384
-20.203056	0.099773	0.405389
-20.204103	3.120846	0.410394
-20.340268	-11.917347	0.415398
-20.249681	-1.025820	0.420403
-20.768352	-5.450647	0.425408
-21.710363	1.562208	0.430413
-21.888279	1.841419	0.435418
-21.809745	-2.566470	0.440422
-21.708624	5.467511	0.445427
-21.745284	3.955421	0.450432
-22.676002	0.898267	0.455437
-23.253719	0.927754	0.460442
-23.331615	1.166327	0.465446
-23.691221	3.456852	0.470451
-23.169876	-1.625641	0.475456
-23.373819	2.932118	0.480461
-23.193718	3.486917	0.485466
-23.877845	2.377257	0.490470
-24.157948	9.183416	0.495475
-24.158218	10.068228	0.500480
-24.923959	10.206207	0.505485
-25.784593	4.225990	0.510490
-25.887583	5.729876	0.515494
-26.385193	4.898354	0.520499
-26.260547	0.936695	0.525504
-26.578723	-0.726109	0.530509
-26.432005	2.142227	0.535514
-26.484942	10.909754	0.540518
-26.482866	11.436018	0.545523
-26.307794	5.222918	0.550528
-27.363350	8.211813	0.555533
-27.605049	1.584463	0.560538
-27.494945	0.797936	0.565542
-28.561351	4.256306	0.570547
-29.086848	-7.046228	0.575552
-29.530382	1.293236	0.580557
-28.805374	3.381850	0.585562
-28.709439	-5.661909	0.590566
-29.160282	0.325566	0.595571
-29.462424	-6.126603	0.600576
-30.117754	11.494974	0.605581
-30.529045	5.822779	0.610586
-30.479562	4.834946	0.615590
-30.846883	11.486238	0.620595
-30.693354	3.069731	0.625600
-30.875213	9.976837	0.630605
-31.515878	7.943565	0.635610
-31.767112	6.503713	0.640614
-32.758108	9.846195	0.645619
-32.332350	6.046606	0.650624
-32.672330	5.795978	0.655629
-32.468038	-2.511322	0.660634
-33.011670	-1.979740	0.665638
-33.008887	3.867694	0.670643
-32.937637	-4.213333	0.675648
-33.639892	13.254598	0.680653
-34.007070	4.997925	0.685658
-33.989155	7.093917	0.690662
-34.596134	3.578225	0.695667
-34.983208	-3.295000	0.700672
-35.520169	7.917324	0.705677
-35.480558	-4.963331	0.710682
-35.794795	3.093650	0.715686
-35.758680	1.902608	0.720691
-35.510863	0.512721	0.725696
-35.621963	10.158737	0.730701
-36.054667	4.672031	0.735706
-36.863744	2.797284	0.740710
-37.371747	3.699676	0.745715
-37.320027	1.236408	0.750720
-37.446470	11.440261	0.755725
-37.620187	-2.927298	0.760730
-38.338091	5.361898	0.765734
-38.991499	16.927795	0.770739
-38.493662	5.844929	0.775744
-38.902777	10.969270	0.780749
-39.217576	11.576424	0.785754
-38.818015	5.257675	0.790758
-39.497743	13.240014	0.795763
-39.117947	2.032250	0.800768
-40.050395	3.978179	0.805773
-40.275978	2.363584	0.810778
-40.589251	4.817920	0.815782
-40.953330	9.147048	0.820787
-40.847833	6.058996	0.825792
-40.977048	5.765374	0.830797
-41.470490	0.603673	0.835802
-41.845251	11.213714	0.840806
-42.124094	3.371023	0.845811
-42.143455	7.295363	0.850816
-42.428868	9.726931	0.855821
-42.553883	13.938722	0.860826
-42.998550	2.954318	0.865830
-43.608012	9.641959	0.870835
-43.414409	6.324420	0.875840
-43.813878	8.996284	0.880845
-43.668991	5.027720	0.885850
-44.065157	2.694665	0.890854
-44.834334	-1.091741	0.895859
-45.294286	0.546443	0.900864
-45.307128	15.685536	0.905869
-45.719150	2.549332	0.910874
-45.495275	7.371711	0.915878
-45.525021	7.215735	0.920883
-45.637372	-2.323767	0.925888
-45.434044	4.547569	0.930893
-46.890589	2.001766	0.935898
-46.931872	13.573639	0.940902
-47.412108	5.048177	0.945907
-46.974258	2.685342	0.950912
-47.112329	4.312056	0.955917
-47.728820	6.331956	0.960922
-47.938314	-2.706610	0.965926
-48.516581	10.432016	0.970931
-48.629454	9.036345	0.975936
-48.587867	2.746094	0.980941
-48.562675	4.998352	0.985946
-49.249934	8.790184	0.990950
-49.634225	11.176165	0.995955
-49.794887	8.366030	1.000960
-49.722118	8.200181	1.005965
-49.957276	6.411545	1.010970
-50.886839	3.119379	1.015974
-51.468697	-1.614856	1.020979
-51.556538	-2.905941	1.025984
-51.739844	0.153404	1.030989
-52.195587	3.433098	1.035994
-51.555511	-7.510119	1.040998
-51.877701	3.691498	1.046003
-51.602794	-1.070959	1.051008
-51.971649	5.737267	1.056013
-52.232599	12.354368	1.061018
-52.951008	0.729765	1.066022
-53.427786	10.639592	1.071027
-53.723009	-3.672913	1.076032
-53.759403	-4.619094	1.081037
-54.381006	-2.486262	1.086042
-54.833928	0.044875	1.091046
-55.123708	4.013405	1.096051
-54.986518	-3.008601	1.101056
-55.239858	3.589870	1.106061
-55.241972	0.557726	1.111066
-54.953999	-1.001020	1.116070
-55.333035	6.863244	1.121075
-55.722428	4.217282	1.126080
-55.962174	-6.264894	1.131085
-56.531772	1.128318	1.136090
-56.582090	-8.118348	1.141094
-56.970664	6.213903	1.146099
-57.895226	3.392143	1.151104
-58.302366	7.191261	1.156109
-58.392978	6.270240	1.161114
-57.545352	-5.690268	1.166118
-58.169745	5.484043	1.171123
-58.266334	3.072173	1.176128
-58.629312	0.358296	1.181133
-59.040248	13.427971	1.186138
-59.403837	-1.459490	1.191142
-60.082213	4.598822	1.196147
-60.209877	7.410378	1.201152
-60.303716	10.100695	1.206157
-60.064017	8.813186	1.211162
-59.959414	16.328592	1.216166
-60.375826	11.815594	1.221171
-60.934897	2.323432	1.226176
-61.341044	7.825372	1.231181
-61.288487	2.805907	1.236186
-61.518227	0.822003	1.241190
-62.109377	11.180957	1.246195
-62.773618	3.827149	1.251200
-63.042603	2.511797	1.256205
-63.238616	4.393392	1.261210
-62.947148	3.589853	1.266214
-63.050871	19.341918	1.271219
-63.264537	10.262992	1.276224
-63.519955	6.926673	1.281229
-64.153587	3.371987	1.286234
-64.170531	0.760843	1.291238
-64.763934	11.672309	1.296243
-64.666194	-2.053678	1.301248
-64.748748	8.785814	1.306253
-65.323797	8.186556	1.311258
-66.094689	4.270987	1.316262
-66.456466	8.070881	1.321267
-66.228445	7.527278	1.326272
-66.221148	7.811141	1.331277
-66.411069	0.148496	1.336282
-66.276698	12.084759	1.341286
-66.779196	5.099819	1.346291
-67.367009	0.522859	1.351296
-67.990695	11.319164	1.356301
-67.897260	5.073410	1.361306
-67.847989	6.307387	1.366310
-68.124454	11.544738	1.371315
-68.263130	4.208874	1.376320
-69.169400	8.915112	1.381325
-69.462417	9.196811	1.386330
-69.410963	0.413201	1.391334
-69.716205	4.519860	1.396339
-69.857449	3.313988	1.401344
-69.895476	-3.460157	1.406349
-70.189184	5.860304	1.411354
-70.677291	-10.131126	1.416358
-70.920212	5.959512	1.421363
-70.976059	-8.643043	1.426368
-71.342960	9.007131	1.431373
-71.339478	2.929010	1.436378
-71.579933	4.100068	1.441382
-72.193929	0.877796	1.446387
-72.247772	0.174462	1.451392
-72.582436	12.122491	1.456397
-72.783823	5.227200	1.461402
-72.778108	4.712322	1.466406
-73.622497	5.483553	1.471411
-74.119787	1.824989	1.476416
-74.395762	2.500702	1.481421
-74.483092	5.885935	1.486426
-74.369994	7.865720	1.491430
-74.759249	-0.035639	1.496435
-74.579524	-6.981609	1.501440
-74.671874	8.161760	1.506445
-74.990559	5.811733	1.511450
-75.418806	2.033794	1.516454
-75.849595	8.499447	1.521459
-75.954124	2.795401	1.526464
-75.973155	6.544650	1.531469
-76.529085	6.110947	1.536474
-77.101639	7.224919	1.541478
-77.440904	11.779241	1.546483
-77.472924	2.617354	1.551488
-77.091107	11.865805	1.556493
-77.544465	1.728422	1.561498
-77.680560	-0.559490	1.566502
-78.710643	13.846053	1.571507
-78.607204	9.367142	1.576512
-79.048896	6.164287	1.581517
-78.864233	6.426669	1.586522
-78.885528	5.618489	1.591526
-79.912421	12.325537	1.596531
-80.534075	-2.573051	1.601536
-80.808696	13.001095	1.606541
-80.727689	6.403580	1.611546
-80.652231	6.616165	1.616550
-80.753251	6.465481	1.621555
-80.521044	7.857615	1.626560
-80.609000	-1.862931	1.631565
-81.651511	3.282441	1.636570
-81.651844	4.581070	1.641574
-82.438549	4.928350	1.646579
-82.676643	6.060142	1.651584
-82.201242	4.497586	1.656589
-82.879665	9.166684	1.661594
-83.438081	6.784728	1.666598
-83.941918	7.337550	1.671603
-83.918508	1.738611	1.676608
-84.226269	2.352693	1.681613
-84.154120	6.937742	1.686618
-84.132576	0.012244	1.691622
-84.449448	2.611033	1.696627
-84.105725	5.011620	1.701632
-84.856773	-3.281317	1.706637
-85.304796	4.730136	1.711642
-85.430708	6.832976	1.716646
-85.793470	13.785631	1.721651
-86.005830	0.217956	1.726656
-86.997387	-2.456540	1.731661
-87.296220	-1.941814	1.736666
-87.079312	2.169933	1.741670
-87.288630	3.484426	1.746675
-86.891987	1.097826	1.751680
-87.341138	6.992477	1.756685
-87.369836	1.427031	1.761690
-87.730851	2.543464	1.766694
-88.370118	1.914589	1.771699
-88.626047	0.689033	1.776704
-89.070031	-0.598716	1.781709
-89.245911	10.122242	1.786714
-89.179087	-8.859519	1.791718
-90.126085	1.494033	1.796723
-90.452051	-0.003688	1.801728
-90.329860	3.199437	1.806733
-90.836129	8.427288	1.811738
-90.597258	-5.090200	1.816742
-90.695209	-3.173539	1.821747
-90.563630	-0.777287	1.826752
-91.076664	-4.148093	1.831757
-91.605705	2.359878	1.836762
-91.580856	-0.948458	1.841766
-92.216585	3.946619	1.846771
-92.028856	0.501195	1.851776
-92.460728	5.476964	1.856781
-93.443697	10.932554	1.861786
-93.686567	-3.677705	1.866790
-93.789381	2.735799	1.871795
-93.803445	1.196881	1.876800
-93.725423	-0.886535	1.881805
-94.369668	-1.285678	1.886810
-93.726283	2.964412	1.891814
-94.105960	3.304865	1.896819
-94.649847	2.286840	1.901824
-95.242545	7.178147	1.906829
-95.219500	-1.383688	1.911834
-95.245805	-0.030636	1.916838
-96.139623	6.475195	1.921843
-96.640739	-5.343244	1.926848
-96.702500	2.129059	1.931853
-96.840795	3.837507	1.936858
-96.974922	-10.353662	1.941862
-97.145101	7.396140	1.946867
-97.123139	-4.956086	1.951872
-97.371698	3.437126	1.956877
-98.172448	7.602960	1.961882
-98.340776	-8.757946	1.966886
-98.637869	-2.542359	1.971891
-98.502090	2.426421	1.976896
-98.520821	-2.263528	1.981901
-98.940908	-3.618182	1.986906
-99.031101	-14.406906	1.991910
-100.184567	-9.341035	1.996915
-100.070765	-5.696540	2.006912
-99.709207	-3.635687	2.016909
-99.060128	-2.160873	2.026906
-98.888640	4.785944	2.036902
-97.795042	2.926776	2.046899
-97.626342	2.262063	2.056896
-97.386816	2.731223	2.066893
-96.344454	5.901196	2.076890
-95.952000	3.707653	2.086886
-95.728975	9.987779	2.096883
-95.379239	3.103707	2.106880
-94.473598	0.071976	2.116877
-94.404836	-1.118163	2.126874
-93.242262	1.324544	2.136870
-92.986559	1.283427	2.146867
-92.899879	3.655953	2.156864
-92.142405	0.569134	2.166861
-91.670571	5.759465	2.176858
-91.332649	0.473252	2.186854
-90.078427	7.085650	2.196851
-89.983584	3.170237	2.206848
-89.690147	-0.611303	2.216845
-89.510862	0.613918	2.226842
-88.513418	0.254743	2.236838
-88.278944	8.076316	2.246835
-87.352201	10.240365	2.256832
-86.981856	-0.331107	2.266829
-86.915057	-2.062503	2.276826
-85.909368	3.665563	2.286822
-85.307906	-0.371689	2.296819
-85.404608	1.530921	2.306816
-84.795316	6.426611	2.316813
-84.250732	8.914962	2.326810
-83.097692	2.553443	2.336806
-83.143835	6.870478	2.346803
-82.526423	3.955045	2.356800
-82.139554	4.833900	2.366797
-81.731604	10.883840	2.376794
-80.974983	12.362978	2.386790
-80.759135	3.632114	2.396787
-79.667607	7.006947	2.406784
-79.201239	9.334970	2.416781
-79.151138	6.034344	2.426778
-78.970467	5.496871	2.436774
-77.896644	4.681074	2.446771
-77.501697	2.934257	2.456768
-77.059918	4.775943	2.466765
-76.738769	4.150001	2.476762
-76.177573	-0.896370	2.486758
-75.876922	10.981946	2.496755
-74.730303	2.278123	2.506752
-74.508425	2.340216	2.516749
-74.362184	3.105991	2.526746
-73.585007	3.243278	2.536742
-73.056326	-3.073321	2.546739
-72.084255	-1.635396	2.556736
-71.838690	-0.983876	2.566733
-71.544050	6.255526	2.576730
-71.461575	8.618081	2.586726
-70.920423	3.892944	2.596723
-70.163983	7.958315	2.606720
-68.911802	5.102941	2.616717
-68.856620	0.507090	2.626714
-68.624074	8.093265	2.636710
-68.491718	6.547807	2.646707
-67.052836	6.547849	2.656704
-66.863253	9.482065	2.666701
-66.815303	3.048084	2.676698
-65.776866	2.851259	2.686694
-65.383802	5.920120	2.696691
-65.205975	7.792875	2.706688
-64.818735	5.288605	2.716685
-63.931387	4.303934	2.726682
-63.753661	1.853330	2.736678
-62.909569	3.064284	2.746675
-62.114430	4.223476	2.756672
-62.037139	5.167038	2.766669
-61.929608	4.127559	2.776666
-60.991298	0.501815	2.786662
-60.330879	-3.461618	2.796659
-60.168997	0.821163	2.806656
-59.070347	3.524808	2.816653
-58.838724	5.489819	2.826650
-58.967838	6.244093	2.836646
-57.907722	8.468454	2.846643
-57.017395	6.865243	2.856640
-56.943518	7.226886	2.866637
-57.092186	11.686962	2.876634
-56.202820	12.186817	2.886630
-55.696067	7.498793	2.896627
-54.593928	7.198556	2.906624
-54.268593	10.214815	2.916621
-54.227162	7.580897	2.926618
-53.871265	3.328243	2.936614
-52.556648	6.528026	2.946611
-52.292027	1.067234	2.956608
-52.287147	0.699160	2.966605
-51.725063	1.788475	2.976602
-51.050948	1.127002	2.986598
-50.545511	3.894707	2.996595
-49.809532	4.222181	3.006592
-49.668367	4.071011	3.016589
-48.808684	0.005029	3.026586
-47.992940	4.281878	3.036582
-47.839257	5.964406	3.046579
-47.885995	0.929997	3.056576
-47.396240	6.353878	3.066573
-46.641368	-0.165756	3.076570
-45.765926	-0.886848	3.086566
-45.286091	-2.822583	3.096563
-44.908055	-3.151685	3.106560
-44.783524	0.466479	3.116557
-43.903570	-7.716002	3.126554
-43.567991	-2.271531	3.136550
-43.117233	1.779460	3.146547
-41.888754	-4.222289	3.156544
-41.600295	-3.536772	3.166541
-41.507069	-1.122452	3.176538
-41.740706	7.260536	3.186534
-40.529671	-1.096118	3.196531
-39.959093	1.582556	3.206528
-38.748749	7.731984	3.216525
-38.963415	2.725977	3.226522
-38.321331	3.311440	3.236518
-38.349407	4.556580	3.246515
-37.435131	7.301236	3.256512
-36.844323	3.664481	3.266509
-36.772561	4.042678	3.276506
-36.174304	3.843080	3.286502
-35.303673	4.093526	3.296499
-35.087979	6.561662	3.306496
-33.953423	1.828754	3.316493
-34.021129	5.516296	3.326490
-33.564377	2.443522	3.336486
-33.041270	5.398183	3.346483
-32.319426	0.056298	3.356480
-32.140364	2.989491	3.366477
-31.226500	1.770248	3.376474
-30.763229	4.831241	3.386470
-30.455502	3.873012	3.396467
-30.156442	4.207048	3.406464
-29.316520	3.348789	3.416461
-28.890410	9.279352	3.426458
-28.489683	3.746426	3.436454
-27.431927	2.475496	3.446451
-27.005787	-0.593393	3.456448
-26.970365	2.688616	3.466445
-26.968117	6.308064	3.476442
-26.144399	-1.978124	3.486438
-25.769211	-0.167095	3.496435
-24.843317	-0.360684	3.506432
-24.629901	-2.102134	3.516429
-23.767088	7.201812	3.526426
-23.107794	-0.599342	3.536422
-22.729216	-4.555418	3.546419
-22.641333	5.649416	3.556416
-22.145895	-1.267475	3.566413
-21.271423	0.632576	3.576410
-21.180537	5.008721	3.586406
-20.260821	1.091266	3.596403
-19.610912	0.489723	3.606400
-19.602545	6.999829	3.616397
-19.045851	0.096899	3.626394
-18.210748	2.783737	3.636390
-17.933422	-1.045319	3.646387
-17.471749	0.972488	3.656384
-16.371863	5.101128	3.666381
-16.376418	4.307435	3.676378
-16.141829	2.186275	3.686374
-15.696030	7.459372	3.696371
-14.823304	4.053740	3.706368
-14.454939	1.837320	3.716365
-13.592987	-2.517902	3.726362
-13.119193	0.996192	3.736358
-13.034184	-1.719036	3.746355
-12.670763	-3.481177	3.756352
-11.988276	7.091103	3.766349
-11.456740	-2.624446	3.776346
-10.531646	0.431994	3.786342
-10.200912	-0.763985	3.796339
-9.831463	-1.407404	3.806336
-9.596861	-2.894117	3.816333
-9.209572	4.641742	3.826330
-8.567507	7.025641	3.836326
-7.453590	1.184933	3.846323
-6.998182	3.776186	3.856320
-6.845367	-1.169755	3.866317
-6.721005	-2.694722	3.876314
-6.262397	4.973960	3.886310
-5.268802	-2.256993	3.896307
-4.881869	0.071745	3.906304
-3.808715	4.498033	3.916301
-3.615212	6.722270	3.926298
-3.265695	7.174210	3.936294
-3.162019	4.348007	3.946291
-2.898437	18.820068	3.956288
-2.484804	29.352516	3.966285
-1.907734	37.751637	3.976282
-1.398776	59.733476	3.986278
-0.971429	75.418525	3.996275
-0.704075	93.622252	4.006272
-0.032105	114.601095	4.016269
0.000000	133.285952	4.021274
0.656257	133.281792	4.026278
0.854039	159.510722	4.031283
1.335917	166.387909	4.036288
1.046102	175.381436	4.041293
0.992613	172.506949	4.046298
1.077054	178.663967	4.051302
1.105638	176.428280	4.056307
0.927962	168.635643	4.061312
0.967296	177.602885	4.066317
1.374141	192.995503	4.071322
1.812317	196.082017	4.076326
1.589777	206.395846	4.081331
1.481409	201.638384	4.086336
1.608946	207.711514	4.091341
1.437450	217.726420	4.096346
1.694688	205.019316	4.101350
1.665080	211.995036	4.106355
1.285681	195.606880	4.111360
1.635598	202.951125	4.116365
1.722384	193.408319	4.121370
1.393786	187.637504	4.126374
1.215920	192.918577	4.131379
1.197116	204.623037	4.136384
1.862865	199.835266	4.141389
1.484192	201.206036	4.146394
1.871967	202.338195	4.151398
1.579503	207.990691	4.156403
1.777306	207.656924	4.161408
1.797829	205.488280	4.166413
1.713063	199.814824	4.171418
2.011231	205.650522	4.176422
1.671456	203.707698	4.181427
1.563861	203.853905	4.186432
1.559751	206.720025	4.191437
1.681436	209.511244	4.196442
1.884677	205.094485	4.201446
1.523767	210.239323	4.206451
1.573937	210.462415	4.211456
1.604979	205.780140	4.216461
1.619698	218.799237	4.221466
1.980516	204.193975	4.226470
1.818777	201.662223	4.231475
1.794683	207.635548	4.236480
2.201024	207.171540	4.241485
1.608073	208.099056	4.246490
1.744345	208.289735	4.251494
1.876723	208.305824	4.256499
1.905546	209.864468	4.261504
2.044624	201.967857	4.266509
1.872552	204.543092	4.271514
2.281767	207.077720	4.276518
1.737642	213.944857	4.281523
1.786688	206.279827	4.286528
1.951162	204.657054	4.291533
1.515733	209.866329	4.296538
1.877686	208.566850	4.301542
1.757506	207.000686	4.306547
1.649571	207.661602	4.311552
2.261374	215.883848	4.316557
2.139239	219.517615	4.321562
1.862068	207.113706	4.326566
2.098963	212.123242	4.331571
2.085914	223.739345	4.336576
2.228446	209.330461	4.341581
1.840790	222.713183	4.346586
2.275244	220.252411	4.351590
2.099898	235.780156	4.356595
2.350734	235.011557	4.361600
2.384298	222.034818	4.366605
2.069129	219.890778	4.371610
1.929949	215.146111	4.376614
2.353331	227.223148	4.381619
2.115797	223.811194	4.386624
2.293082	231.869190	4.391629
2.171213	235.100548	4.396634
2.558868	231.941850	4.401638
2.349780	223.791090	4.406643
1.993221	213.391838	4.411648
2.024204	216.152297	4.416653
2.384807	233.841514	4.421658
2.528272	243.593526	4.426662
2.266924	242.377524	4.431667
2.324304	237.750276	4.436672
2.632706	232.556548	4.441677
2.209685	233.987155	4.446682
2.304553	232.338018	4.451686
2.516534	234.179705	4.456691
2.323295	241.653773	4.461696
2.574315	240.928163	4.466701
2.256492	248.558040	4.471706
2.439588	238.222739	4.476710
2.254426	250.081274	4.481715
2.340888	249.021392	4.486720
2.349770	239.554408	4.491725
2.238213	238.990466	4.496730
2.546024	239.167343	4.501734
2.315087	242.702901	4.506739
2.515847	243.643436	4.511744
2.409673	246.431348	4.516749
2.059689	239.815508	4.521754
2.570171	245.235401	4.526758
2.513070	243.038560	4.531763
2.665769	245.513649	4.536768
2.207811	232.748535	4.541773
2.078366	248.417089	4.546778
2.491349	247.480740	4.551782
2.691836	263.540655	4.556787
2.743757	261.111056	4.561792
2.752111	263.313058	4.566797
2.967349	272.049352	4.571802
3.107312	257.377996	4.576806
2.655330	254.097847	4.581811
2.798775	246.936950	4.586816
3.042450	241.996266	4.591821
2.698762	245.019660	4.596826
2.717548	239.728254	4.601830
2.317206	245.158272	4.606835
2.622303	246.891004	4.611840
2.671202	234.973977	4.616845
2.947717	260.512782	4.621850
2.969967	250.611213	4.626854
2.769809	241.716191	4.631859
2.511801	243.111975	4.636864
2.997234	253.240716	4.641869
2.595146	272.822831	4.646874
3.169572	264.155525	4.651878
3.146614	267.767947	4.656883
2.862946	259.130848	4.661888
2.979973	237.014842	4.666893
2.368154	248.624343	4.671898
2.740480	248.553535	4.676902
2.902925	263.113480	4.681907
2.607582	269.928394	4.686912
3.333982	270.114496	4.691917
3.169540	279.029503	4.696922
3.392194	259.906347	4.701926
3.094034	262.996207	4.706931
3.136869	267.619938	4.711936
3.301049	271.241037	4.716941
3.112669	269.114081	4.721946
3.175952	248.828771	4.726950
2.626972	252.179009	4.731955
3.043155	260.780590	4.736960
3.234781	267.251617	4.741965
2.977822	279.203366	4.746970
3.015171	265.286246	4.751974
3.158910	276.221859	4.756979
3.365723	261.920289	4.761984
3.133261	268.082854	4.766989
3.083139	271.615512	4.771994
2.998240	265.184084	4.776998
3.248547	267.457713	4.782003
3.028196	269.336659	4.787008
3.106749	269.071182	4.792013
3.067263	272.471245	4.797018
3.068666	274.657034	4.802022
3.081629	273.713121	4.807027
3.009203	275.235651	4.812032
3.043738	271.015138	4.817037
3.293186	277.787006	4.822042
3.186102	274.600702	4.827046
3.186494	270.006562	4.832051
2.892669	273.561618	4.837056
3.479698	284.160979	4.842061
3.281634	296.067665	4.847066
3.528494	290.778138	4.852070
3.288582	304.393200	4.857075
3.241055	301.115923	4.862080
3.516773	302.289142	4.867085
3.393960	312.385244	4.872090
3.748698	306.037881	4.877094
3.442109	299.842064	4.882099
3.573251	304.609645	4.887104
3.689844	294.021085	4.892109
3.548962	286.418645	4.897114
3.294742	272.483100	4.902118
3.041061	285.541962	4.907123
3.593218	294.633728	4.912128
3.580603	302.714919	4.917133
3.529899	299.137230	4.922138
3.726471	304.507891	4.927142
3.392210	306.671715	4.932147
3.486573	303.231424	4.937152
3.308684	300.872631	4.942157
3.205410	303.100820	4.947162
3.597876	298.730451	4.952166
3.358006	302.052602	4.957171
3.550890	302.780729	4.962176
3.407713	299.615000	4.967181
2.959794	308.399164	4.972186
3.367157	319.176894	4.977190
3.730736	324.689223	4.982195
3.648130	333.963875	4.987200
4.413136	332.245198	4.992205
3.815182	333.389436	4.997210
3.965955	319.921964	5.002214
3.539722	311.830598	5.007219
3.763861	314.113304	5.012224
3.808354	307.593929	5.017229
4.052603	311.694924	5.022234
3.732874	315.497399	5.027238
3.364735	314.327492	5.032243
4.264058	322.000356	5.037248
4.241934	315.397286	5.042253
3.643491	313.448539	5.047258
3.933786	306.602323	5.052262
3.858725	315.313895	5.057267
3.810958	321.030896	5.062272
3.929954	307.120938	5.067277
3.457675	313.811839	5.072282
4.020234	320.571937	5.077286
3.990786	335.935710	5.082291
3.565396	341.590533	5.087296
3.983432	332.683273	5.092301
3.748643	336.616533	5.097306
3.905488	332.172097	5.102310
4.099527	344.897964	5.107315
3.775558	337.221623	5.112320
4.009659	336.879079	5.117325
3.896142	338.003089	5.122330
4.078398	337.254327	5.127334
4.152467	335.152773	5.132339
4.073427	332.948304	5.137344
4.323946	339.379022	5.142349
4.011995	334.591491	5.147354
4.343465	336.969305	5.152358
4.292647	332.603065	5.157363
4.247714	329.870991	5.162368
4.115893	337.950036	5.167373
4.070857	340.168586	5.172378
4.142476	336.345075	5.177382
4.282106	332.089579	5.182387
3.989427	333.586624	5.187392
4.234019	326.299813	5.192397
3.593101	346.508253	5.197402
3.865031	338.718040	5.202406
4.139462	345.360490	5.207411
4.123465	363.999646	5.212416
4.580095	363.431993	5.217421
4.164916	373.112804	5.222426
4.502093	368.761240	5.227430
4.490670	373.756892	5.232435
4.498051	358.893678	5.237440
4.284226	346.726431	5.242445
4.232376	346.483139	5.247450
4.437928	352.634380	5.252454
4.396379	356.281869	5.257459
4.114654	372.829646	5.262464
4.553063	362.467969	5.267469
4.198177	372.862631	5.272474
4.111259	366.932141	5.277478
4.222169	366.871272	5.282483
4.287901	374.205627	5.287488
4.609559	365.236557	5.292493
4.429073	373.843072	5.297498
4.618250	375.075028	5.302502
4.535310	374.305452	5.307507
4.699866	374.801666	5.312512
4.699412	365.414494	5.317517
4.585649	382.895109	5.322522
4.815533	370.402368	5.327526
4.919386	373.043435	5.332531
4.691944	364.245214	5.337536
4.980424	368.784095	5.342541
4.435036	362.526562	5.347546
4.699415	363.301462	5.352550
4.925861	356.017839	5.357555
4.401071	349.879842	5.362560
4.494457	359.748558	5.367565
4.572101	367.575467	5.372570
4.855642	374.161759	5.377574
4.737700	364.087967	5.382579
5.034118	375.141833	5.387584
4.712039	347.017016	5.392589
4.395689	355.925450	5.397594
4.468592	366.779516	5.402598
4.541478	375.421827	5.407603
4.507185	382.462337	5.412608
4.447406	369.296884	5.417613
4.598779	374.742149	5.422618
4.995317	375.394326	5.427622
4.922540	377.447370	5.432627
5.064948	370.263499	5.437632
5.119813	364.011551	5.442637
4.904505	380.304428	5.447642
4.654864	366.139917	5.452646
4.806672	379.877650	5.457651
4.409936	380.475887	5.462656
5.024344	369.101331	5.467661
4.530530	372.612170	5.472666
5.002995	371.070004	5.477670
4.801540	378.840321	5.482675
4.786858	376.625781	5.487680
4.967183	369.213034	5.492685
4.574133	385.964757	5.497690
4.843327	395.108175	5.502694
4.867666	405.698575	5.507699
4.704477	408.877412	5.512704
5.059305	404.955285	5.517709
4.850677	406.651149	5.522714
4.883890	402.518635	5.527718
5.018924	410.022688	5.532723
4.950785	404.728056	5.537728
5.391935	405.560713	5.542733
4.955918	407.492359	5.547738
5.153884	402.121299	5.552742
4.922992	403.025970	5.557747
4.755069	408.261463	5.562752
4.993938	399.738254	5.567757
4.895809	402.161759	5.572762
5.397079	418.994337	5.577766
5.349164	415.025626	5.582771
4.967781	409.622230	5.587776
5.604150	410.689954	5.592781
5.205226	418.437143	5.597786
5.094783	404.033067	5.602790
5.207191	418.326749	5.607795
5.293608	427.247464	5.612800
5.472574	416.460823	5.617805
5.504014	410.218262	5.622810
5.488241	401.025418	5.627814
5.067603	398.835669	5.632819
5.135127	401.855727	5.637824
5.783225	407.210068	5.642829
5.185000	399.807628	5.647834
5.378807	399.780788	5.652838
5.462043	407.126666	5.657843
5.496739	396.589881	5.662848
5.490394	394.211153	5.667853
5.560551	402.512733	5.672858
5.248087	397.541151	5.677862
5.643622	404.510099	5.682867
5.419224	403.565818	5.687872
5.407915	395.282758	5.692877
5.205055	407.098364	5.697882
5.629527	420.733755	5.702886
5.536373	423.291813	5.707891
5.495736	434.189001	5.712896
5.650397	425.703204	5.717901
5.512459	433.457703	5.722906
5.547800	430.256465	5.727910
5.593283	430.229124	5.732915
5.020542	430.886503	5.737920
5.623561	432.935197	5.742925
5.500231	433.581897	5.747930
5.703522	431.013144	5.752934
5.942915	437.680974	5.757939
5.451369	434.235652	5.762944
5.736607	425.785658	5.767949
5.485918	436.224678	5.772954
5.550736	432.796158	5.777958
5.525229	428.442474	5.782963
5.483503	433.316669	5.787968
5.873998	437.055637	5.792973
5.510612	440.825903	5.797978
5.553460	435.200297	5.802982
5.288506	432.408337	5.807987
5.350480	447.033835	5.812992
6.073092	452.658245	5.817997
5.746542	451.123270	5.823002
6.082905	453.763739	5.828006
5.876700	442.516925	5.833011
5.459936	435.734454	5.838016
5.928617	457.830763	5.843021
5.614397	465.109478	5.848026
5.593820	462.235406	5.853030
5.998566	461.644373	5.858035
5.942038	454.102082	5.863040
6.192917	460.310390	5.868045
5.960511	468.302161	5.873050
5.892241	469.918745	5.878054
6.033374	465.945554	5.883059
5.768427	461.544286	5.888064
5.919221	455.399951	5.893069
5.878554	466.343146	5.898074
5.897345	461.683148	5.903078
5.975299	461.688912	5.908083
5.700879	474.517322	5.913088
5.746694	462.797378	5.918093
5.989692	473.274654	5.923098
5.861841	469.581627	5.928102
5.985295	466.820658	5.933107
5.600679	464.714724	5.938112
5.903510	475.323981	5.943117
6.326801	486.276599	5.948122
6.354584	484.936132	5.953126
5.990494	481.778727	5.958131
6.060129	500.142195	5.963136
6.217494	493.634244	5.968141
6.386899	493.498566	5.973146
6.292361	473.217586	5.978150
6.148683	469.208279	5.983155
6.058201	464.519606	5.988160
6.219672	477.683937	5.993165
5.926826	493.494450	5.998170
6.395195	497.205934	6.003174
6.127430	490.678988	6.008179
6.606845	498.433315	6.013184
6.533128	488.801658	6.018189
6.160096	495.356812	6.023194
6.220737	495.380835	6.028198
6.048206	497.046655	6.033203
5.876729	501.912165	6.038208
6.421073	496.643166	6.043213
5.983853	499.753139	6.048218
6.242955	498.937376	6.053222
6.390744	497.667023	6.058227
6.385317	506.364803	6.063232
6.630628	501.830287	6.068237
6.413924	505.210609	6.073242
6.221934	506.948524	6.078246
6.484808	495.624194	6.083251
6.132364	507.748223	6.088256
6.234064	496.388616	6.093261
6.096362	505.064490	6.098266
6.399000	497.426590	6.103270
6.289761	499.738874	6.108275
6.408891	505.448040	6.113280
6.689634	492.943227	6.118285
6.317783	506.019869	6.123290
5.921332	506.180362	6.128294
6.312891	501.594593	6.133299
6.110903	504.415782	6.138304
6.085471	498.989722	6.143309
6.193813	505.059833	6.148314
6.230515	505.230694	6.153318
6.132870	512.353979	6.158323
6.207615	515.623090	6.163328
6.499001	507.770566	6.168333
6.318552	512.482258	6.173338
6.549401	509.719285	6.178342
6.620681	504.173013	6.183347
6.609547	508.729975	6.188352
6.824225	503.615417	6.193357
6.649118	508.225580	6.198362
6.661370	494.612366	6.203366
6.235708	480.529588	6.208371
5.962989	477.672994	6.213376
6.073606	479.338498	6.218381
6.402113	493.242438	6.223386
6.159697	496.580641	6.228390
6.327767	495.270027	6.233395
6.227300	503.792914	6.238400
6.033998	498.888396	6.243405
6.555593	502.513118	6.248410
6.382836	502.604009	6.253414
6.495803	502.625484	6.258419
6.286936	507.878644	6.263424
6.537183	492.028645	6.268429
6.266853	485.551065	6.273434
6.306369	469.630407	6.278438
6.550831	471.815443	6.283443
6.079163	470.536764	6.288448
6.053668	465.205055	6.293453
6.198994	478.536246	6.298458
6.282376	495.571311	6.303462
6.213180	502.107137	6.308467
6.203848	508.410651	6.313472
6.657129	496.940925	6.318477
6.246250	493.707199	6.323482
6.027876	498.659211	6.328486
6.752320	489.043193	6.333491
6.431243	486.567577	6.338496
6.722934	476.655189	6.343501
6.078011	477.024566	6.348506
5.930139	465.624808	6.353510
5.576629	476.808865	6.358515
5.718795	494.286891	6.363520
6.420392	496.268554	6.368525
6.477732	496.818047	6.373530
6.230942	494.314933	6.378534
6.549005	499.108652	6.383539
6.415807	500.320788	6.388544
6.334206	492.726191	6.393549
6.377547	500.738623	6.398554
6.565942	498.684423	6.403558
6.487706	494.622634	6.408563
6.550422	503.649342	6.413568
6.425977	498.311115	6.418573
6.111391	484.723812	6.423578
5.788488	490.132014	6.428582
6.342365	497.910715	6.433587
6.228856	498.062245	6.438592
6.821981	486.655410	6.443597
6.763251	501.949208	6.448602
6.569440	488.224880	6.453606
6.560473	483.106119	6.458611
6.168491	475.855976	6.463616
6.434740	461.974185	6.468621
6.043719	473.407771	6.473626
6.253890	464.572351	6.478630
6.188473	464.102982	6.483635
6.098266	468.269072	6.488640
6.392649	464.187227	6.493645
6.230176	469.156417	6.498650
6.247935	463.822281	6.503654
6.460750	473.357722	6.508659
6.429249	475.528267	6.513664
6.296813	459.601164	6.518669
6.285194	461.377486	6.523674
6.023970	467.317360	6.528678
6.168543	476.994347	6.533683
6.190971	493.357301	6.538688
6.771058	498.828710	6.543693
6.316867	485.454168	6.548698
6.509521	477.264573	6.553702
6.311207	468.126190	6.558707
5.992920	461.105393	6.563712
6.547481	473.921841	6.568717
6.037466	467.449228	6.573722
5.830105	478.411943	6.578726
6.304815	491.375228	6.583731
6.723417	509.433259	6.588736
6.676735	486.333430	6.593741
6.097898	476.722276	6.598746
6.527601	469.966176	6.603750
6.482987	475.381966	6.608755
6.410083	468.355068	6.613760
6.674736	474.474863	6.618765
6.545167	477.859695	6.623770
6.162854	476.099709	6.628774
6.401205	468.043256	6.633779
6.451875	467.828767	6.638784
6.400019	462.478335	6.643789
6.424648	464.637611	6.648794
6.266250	470.144862	6.653798
6.567474	467.845831	6.658803
5.947683	477.130388	6.663808
6.256709	463.329526	6.668813
6.576561	471.806672	6.673818
6.593327	471.174505	6.678822
6.610621	466.545144	6.683827
6.506491	463.994336	6.688832
6.538166	471.143156	6.693837
6.275532	475.701694	6.698842
6.510311	469.223164	6.703846
6.410997	460.333024	6.708851
5.929614	450.118468	6.713856
6.521601	457.377362	6.718861
6.443902	462.731531	6.723866
6.215346	449.864707	6.728870
6.049560	445.466757	6.733875
6.255600	453.760073	6.738880
6.628956	466.524230	6.743885
6.216365	463.326907	6.748890
6.328888	457.948073	6.753894
6.472053	450.897638	6.758899
6.069009	456.251806	6.763904
6.099293	457.515606	6.768909
6.179334	465.547597	6.773914
6.421264	467.092686	6.778918
6.375813	467.702416	6.783923
5.892233	475.201585	6.788928
6.390411	467.313260	6.793933
6.189177	472.508705	6.798938
6.257479	478.826387	6.803942
6.622874	460.178222	6.808947
6.101800	472.058016	6.813952
6.222750	460.944685	6.818957
6.247034	464.585640	6.823962
6.442957	462.312729	6.828966
6.475598	463.841758	6.833971
6.606804	464.359876	6.838976
6.441492	463.719182	6.843981
6.582724	460.236955	6.848986
6.056039	448.011518	6.853990
6.354729	446.355445	6.858995
6.299369	452.706223	6.864000
6.768718	448.220663	6.869005
6.091089	439.004191	6.874010
6.528968	437.442487	6.879014
6.317305	430.627633	6.884019
6.107979	435.937284	6.889024
6.749212	432.518299	6.894029
6.395545	426.354894	6.899034
6.336972	434.378050	6.904038
6.417096	433.014515	6.909043
5.681863	440.110340	6.914048
6.256063	434.037590	6.919053
5.953213	435.915022	6.924058
6.187353	455.658420	6.929062
6.386481	456.521290	6.934067
6.098290	469.435056	6.939072
6.305528	457.049993	6.944077
6.460751	468.813060	6.949082
6.297306	462.466585	6.954086
6.515221	465.874191	6.959091
6.155097	467.256513	6.964096
6.108973	462.492611	6.969101
6.323594	464.177004	6.974106
6.534042	459.077568	6.979110
6.630474	462.733808	6.984115
6.215958	458.937881	6.989120
6.387244	447.000226	6.994125
6.349737	437.491666	6.999130
6.030726	440.518510	7.004134
6.287801	439.576592	7.009139
6.017609	463.260501	7.014144
6.434646	469.941554	7.019149
6.484787	464.455630	7.024154
6.615960	467.902859	7.029158
6.270037	444.251549	7.034163
6.007131	443.151627	7.039168
6.305767	454.363053	7.044173
6.581386	459.530049	7.049178
6.168484	455.526057	7.054182
6.249503	449.927081	7.059187
5.822062	465.716044	7.064192
5.966836	453.348235	7.069197
6.280592	469.463215	7.074202
5.965461	464.693733	7.079206
6.351753	468.087666	7.084211
6.220425	464.228267	7.089216
6.430269	463.881055	7.094221
6.606170	468.287642	7.099226
6.264693	461.558604	7.104230
6.455728	463.174479	7.109235
6.251793	465.110524	7.114240
6.322592	462.849255	7.119245
6.437574	467.491094	7.124250
6.314589	469.531546	7.129254
6.453630	467.131495	7.134259
6.300735	462.382510	7.139264
6.603606	466.858651	7.144269
6.735334	467.226507	7.149274
6.232163	461.570931	7.154278
6.327556	446.662472	7.159283
6.307247	442.743055	7.164288
6.236751	436.225104	7.169293
6.185758	451.625319	7.174298
6.206573	456.686109	7.179302
6.482379	461.569302	7.184307
6.261317	461.643524	7.189312
6.345844	454.886571	7.194317
6.302006	451.452359	7.199322
6.244835	457.351730	7.204326
6.364691	462.599775	7.209331
6.381597	474.223143	7.214336
6.600061	465.930019	7.219341
6.416472	452.063130	7.224346
6.102661	443.694959	7.229350
6.384800	441.540583	7.234355
6.112787	434.737892	7.239360
6.348738	439.588407	7.244365
6.272726	443.983619	7.249370
6.187287	451.794752	7.254374
6.518197	457.903175	7.259379
6.290779	458.335436	7.264384
6.335002	443.913802	7.269389
6.160429	446.437197	7.274394
6.448673	450.377414	7.279398
6.571401	430.495645	7.284403
6.110810	443.762363	7.289408
6.069249	439.117695	7.294413
6.125298	447.057545	7.299418
6.452617	459.884773	7.304422
6.535851	468.833074	7.309427
6.465087	453.128823	7.314432
6.480033	439.271301	7.319437
6.474237	436.059508	7.324442
6.175990	443.110798	7.329446
6.261378	435.049498	7.334451
6.100661	439.275407	7.339456
6.197309	434.293295	7.344461
6.351806	445.236324	7.349466
6.463767	448.700149	7.354470
6.471249	448.068731	7.359475
6.042446	437.468165	7.364480
6.320653	429.123529	7.369485
6.184901	442.836907	7.374490
6.018955	448.591680	7.379494
6.495048	452.427776	7.384499
6.410274	456.033902	7.389504
6.285861	455.123777	7.394509
6.528266	446.358808	7.399514
6.448331	447.109030	7.404518
6.345927	446.099552	7.409523
5.455255	445.754209	7.414528
6.235198	451.463650	7.419533
6.407319	468.312503	7.424538
6.589895	471.557632	7.429542
6.727944	462.667258	7.434547
6.321613	459.254983	7.439552
6.278757	456.572667	7.444557
6.335413	446.009912	7.449562
6.494275	451.937840	7.454566
6.272253	442.596784	7.459571
6.185010	450.264553	7.464576
6.500183	444.093002	7.469581
6.276628	449.861657	7.474586
6.027470	449.348514	7.479590
6.760381	443.206262	7.484595
6.533936	439.607123	7.489600
6.533692	442.370819	7.494605
6.403793	447.535104	7.499610
6.158543	437.264089	7.504614
6.680883	444.873933	7.509619
6.197974	443.685132	7.514624
6.459183	441.274919	7.519629
6.290079	441.584645	7.524634
6.219851	449.365632	7.529638
6.236893	450.233591	7.534643
6.215540	446.298757	7.539648
6.434659	437.330640	7.544653
6.572649	444.833629	7.549658
6.448332	437.705142	7.554662
6.513896	429.948859	7.559667
6.599837	445.984714	7.564672
6.535503	437.161810	7.569677
6.515682	442.095332	7.574682
6.428830	434.143857	7.579686
6.314566	413.062066	7.584691
6.244093	406.827897	7.589696
6.479104	402.872724	7.594701
6.176782	402.671498	7.599706
6.115514	402.951133	7.604710
6.558750	419.167562	7.609715
6.305596	420.552690	7.614720
6.057959	408.144913	7.619725
6.193399	414.075521	7.624730
6.358090	433.870056	7.629734
6.766079	429.965365	7.634739
6.275309	416.710014	7.639744
6.249636	414.205227	7.644749
6.147641	407.140548	7.649754
6.233275	401.263762	7.654758
6.459855	410.083506	7.659763
6.496781	413.750378	7.664768
6.559827	398.621171	7.669773
6.214142	406.259093	7.674778
5.898487	408.998446	7.679782
6.269345	407.643800	7.684787
6.258369	428.266835	7.689792
6.263114	420.593248	7.694797
6.234841	427.463070	7.699802
6.392914	443.217808	7.704806
6.373292	429.945800	7.709811
6.253530	439.252124	7.714816
6.421414	433.109507	7.719821
6.585353	426.550766	7.724826
6.324658	420.500041	7.729830
6.341070	410.175058	7.734835
6.167117	412.077714	7.739840
6.312759	410.543487	7.744845
6.084734	416.691562	7.749850
6.061862	427.206518	7.754854
6.638997	427.238552	7.759859
6.324753	438.067776	7.764864
6.198378	422.228313	7.769869
6.185285	427.836009	7.774874
6.073209	445.317007	7.779878
6.374414	435.052991	7.784883
6.140545	443.342578	7.789888
6.280162	439.749720	7.794893
6.700782	449.313094	7.799898
6.360240	448.200176	7.804902
6.478577	437.527359	7.809907
6.056995	434.528081	7.814912
6.396242	431.519837	7.819917
6.518439	428.425976	7.824922
6.120081	426.682072	7.829926
6.403759	432.424743	7.834931
6.315288	448.026920	7.839936
6.224772	432.840226	7.844941
6.286240	440.881792	7.849946
6.314144	446.070662	7.854950
6.493040	444.661563	7.859955
6.007499	435.951625	7.864960
6.080690	443.811870	7.869965
6.152338	447.617058	7.874970
6.149113	447.224614	7.879974
6.143108	450.725341	7.884979
6.075945	443.952070	7.889984
6.481295	448.519377	7.894989
6.537949	444.673848	7.899994
6.258285	447.224117	7.904998
6.266222	441.748742	7.910003
6.648779	444.408398	7.915008
6.039925	442.877150	7.920013
6.630387	438.380220	7.925018
6.416217	443.355594	7.930022
6.510594	442.772541	7.935027
6.539042	446.498053	7.940032
6.398474	437.458465	7.945037
6.125357	419.540856	7.950042
6.053714	429.465953	7.955046
6.361401	433.676063	7.960051
5.965488	441.655034	7.965056
6.246715	440.242212	7.970061
6.047382	438.722877	7.975066
6.286900	450.635367	7.980070
6.622535	441.593291	7.985075
6.275312	438.774301	7.990080
6.313623	433.949657	7.995085
6.544349	441.920767	8.000090
6.212887	444.313256	8.005094
6.368619	439.639666	8.010099
6.347049	442.425839	8.015104
6.139668	442.869977	8.020109
6.122171	442.746092	8.025126
6.242080	444.253999	8.030144
6.194554	439.259417	8.035162
6.128836	449.073027	8.040179
6.471943	441.788926	8.045197
6.400594	442.914952	8.050214
6.324996	444.422755	8.055232
6.402061	445.158878	8.060250
6.088851	446.687526	8.065267
6.497959	446.539791	8.070285
6.320287	441.039240	8.075302
5.958098	444.077853	8.080320
6.130786	445.332550	8.085338
6.037110	443.938448	8.090355
6.171022	446.869519	8.095373
6.063173	445.265575	8.100390
5.941562	459.412335	8.105408
6.603486	464.587494	8.110426
6.142430	468.512497	8.115443
6.300982	469.184738	8.120461
6.653781	470.174393	8.125478
6.352868	472.521419	8.130496
6.592823	466.878677	8.135514
6.455331	476.389056	8.140531
6.395205	472.947420	8.145549
7.043658	468.880810	8.150566
6.288969	465.234725	8.155584
6.324607	444.241539	8.160602
6.586841	451.716963	8.165619
6.173051	458.640802	8.170637
6.632215	460.773977	8.175654
6.406054	466.243824	8.180672
6.088495	463.520359	8.185690
6.496442	466.088363	8.190707
6.613053	473.549134	8.195725
6.547705	473.236479	8.200742
6.423967	481.997002	8.205760
6.524884	466.045758	8.210778
6.720430	475.714949	8.215795
6.659999	476.881293	8.220813
6.570281	452.588429	8.225830
6.368512	448.205365	8.230848
6.696236	463.273710	8.235866
6.549194	459.830722	8.240883
6.349880	451.408576	8.245901
6.634237	452.148363	8.250918
6.383796	469.855374	8.255936
6.642092	465.758890	8.260954
6.703108	478.696576	8.265971
5.909740	468.928802	8.270989
6.243095	468.767826	8.276006
6.103188	472.690828	8.281024
6.537059	464.358298	8.286042
6.725424	474.704414	8.291059
6.464878	478.704870	8.296077
6.527501	464.654516	8.301094
6.425097	475.527487	8.306112
6.883955	469.515252	8.311130
6.721820	469.809526	8.316147
6.859217	479.257459	8.321165
7.106552	458.926982	8.326182
6.816335	469.938325	8.331200
6.740127	462.802383	8.336218
6.636199	458.765686	8.341235
6.553394	466.409071	8.346253
6.901333	459.456617	8.351270
6.777059	481.463884	8.356288
6.674421	472.922182	8.361306
6.810072	462.057730	8.366323
6.487696	470.457073	8.371341
6.764406	461.101435	8.376358
6.692273	478.721847	8.381376
6.891960	472.551361	8.386394
6.663692	453.792057	8.391411
6.550698	449.461807	8.396429
6.757737	445.862165	8.401446
6.323287	456.030321	8.406464
6.525294	466.750917	8.411482
6.744615	471.966695	8.416499
6.750313	474.653865	8.421517
6.780482	482.673207	8.426534
6.564045	479.786942	8.431552
6.777846	470.088985	8.436570
6.559213	474.356888	8.441587
6.516666	471.063905	8.446605
6.429255	468.467671	8.451622
6.491795	482.922122	8.456640
6.986793	475.083365	8.461658
6.732113	472.746308	8.466675
6.493238	475.797969	8.471693
6.527558	480.397188	8.476710
6.721615	482.757127	8.481728
6.684097	474.395965	8.486746
6.818074	472.765358	8.491763
6.521604	476.987692	8.496781
7.149977	470.182679	8.501798
6.949061	477.260631	8.506816
6.655365	478.875414	8.511834
6.934803	466.341994	8.516851
7.025897	480.262227	8.521869
7.129384	477.954435	8.526886
6.698283	476.031209	8.531904
6.852884	474.719210	8.536922
6.974933	483.826997	8.541939
6.478230	477.033297	8.546957
6.967525	470.820564	8.551974
6.731021	478.568928	8.556992
6.756898	474.278269	8.562010
6.895498	473.296455	8.567027
6.532091	467.336333	8.572045
6.859329	469.747439	8.577063
6.753274	485.832449	8.582080
7.159509	497.693965	8.587098
7.033295	493.941638	8.592115
6.659138	482.905311	8.597133
7.314331	477.555590	8.602151
6.760789	492.469128	8.607168
6.903405	470.733835	8.612186
6.780616	480.287448	8.617203
6.649312	501.466835	8.622221
7.272622	494.044190	8.627239
7.118814	504.040718	8.632256
7.085583	483.764344	8.637274
6.923013	473.556704	8.642291
6.412554	480.589662	8.647309
6.913394	488.770420	8.652327
6.909607	506.467139	8.657344
6.889092	504.868804	8.662362
7.294222	505.968292	8.667379
6.740935	508.378372	8.672397
7.000664	502.431183	8.677415
6.872282	503.878053	8.682432
6.912703	503.697675	8.687450
7.141758	511.063866	8.692467
6.926660	507.743153	8.697485
7.040244	498.109408	8.702503
6.868920	508.817843	8.707520
6.755310	504.464650	8.712538
7.115101	508.892275	8.717555
6.867380	512.590440	8.722573
7.046077	507.931183	8.727591
6.821308	509.698323	8.732608
6.841524	496.446835	8.737626
7.292986	500.047918	8.742643
6.900042	512.692524	8.747661
7.313336	505.248356	8.752679
6.932022	505.055931	8.757696
6.827460	510.270044	8.762714
6.983411	512.013704	8.767731
6.780227	506.266191	8.772749
6.757442	519.586266	8.777767
6.833144	524.301865	8.782784
7.261204	530.835759	8.787802
7.461893	532.714523	8.792819
7.291323	533.671172	8.797837
7.547808	535.191312	8.802855
7.258937	521.840601	8.807872
7.112764	520.588640	8.812890
7.070933	512.703335	8.817907
6.798548	523.480086	8.822925
7.351373	530.062803	8.827943
7.534444	528.025073	8.832960
7.116335	519.808203	8.837978
7.315538	505.123821	8.842995
7.103587	504.049868	8.848013
7.056595	509.405421	8.853031
7.308056	518.218786	8.858048
7.271819	519.395102	8.863066
7.604386	515.648682	8.868083
7.463894	513.122643	8.873101
7.500563	507.785577	8.878119
7.487010	508.712287	8.883136
7.201639	512.696785	8.888154
7.402821	503.625262	8.893171
7.028422	509.534995	8.898189
7.076336	508.205230	8.903207
7.073199	501.002844	8.908224
7.053047	504.593054	8.913242
7.138681	503.508403	8.918259
7.085293	507.712538	8.923277
7.472593	507.130847	8.928295
7.193865	508.385306	8.933312
7.167474	518.558367	8.938330
7.827996	523.949708	8.943347
7.283161	519.292157	8.948365
7.321065	506.981562	8.953383
7.356444	509.339830	8.958400
7.224852	503.533419	8.963418
7.458187	501.546027	8.968435
7.224733	501.802508	8.973453
7.417396	501.492794	8.978471
7.513088	510.677593	8.983488
7.220776	505.729233	8.988506
7.569488	503.347958	8.993523
7.022028	512.553242	8.998541
7.597890	518.350502	9.003559
7.469603	508.811129	9.008576
7.207943	508.119790	9.013594
7.514144	521.363146	9.018611
7.273403	505.238730	9.023629
7.809899	504.040644	9.028647
7.363827	507.898613	9.033664
7.158996	503.688075	9.038682
7.442113	515.556214	9.043699
7.531361	521.112030	9.048717
7.466715	520.054822	9.053735
7.478164	514.985100	9.058752
7.038113	513.866836	9.063770
7.553107	519.736967	9.068787
7.495762	528.661706	9.073805
7.535117	526.590298	9.078823
7.937227	533.860919	9.083840
7.461988	528.022828	9.088858
7.651814	508.096270	9.093875
7.470968	515.057145	9.098893
7.337606	518.308649	9.103911
7.256423	515.840894	9.108928
7.446049	530.017671	9.113946
7.609457	529.074656	9.118963
7.693905	538.076701	9.123981
7.799527	529.666217	9.128999
7.466479	533.506264	9.134016
7.399125	518.695352	9.139034
7.654411	520.118058	9.144051
7.499614	522.685760	9.149069
7.396069	528.589623	9.154087
7.674004	528.858463	9.159104
7.443035	537.786566	9.164122
7.838308	529.588927	9.169139
7.590124	526.334118	9.174157
7.552643	527.801761	9.179175
7.244081	528.661977	9.184192
7.764026	535.640665	9.189210
7.690302	528.248984	9.194227
7.863463	534.529834	9.199245
7.792716	540.802654	9.204263
7.518400	528.993514	9.209280
7.046234	526.791274	9.214298
7.564064	529.958373	9.219315
7.439190	541.076826	9.224333
7.947520	532.810861	9.229351
7.768222	532.962319	9.234368
7.806143	536.570476	9.239386
7.991472	531.748511	9.244403
8.136606	537.129736	9.249421
7.366056	527.854174	9.254439
7.846161	521.858281	9.259456
7.574779	531.751273	9.264474
7.841274	532.135385	9.269491
7.652490	537.729373	9.274509
7.464792	525.098469	9.279527
7.830343	532.598553	9.284544
7.383088	537.292297	9.289562
7.782680	534.028638	9.294579
7.487446	522.984725	9.299597
7.258888	529.215960	9.304615
7.465486	534.896827	9.309632
7.509095	530.524481	9.314650
7.909121	529.474179	9.319667
7.582891	528.404582	9.324685
7.639955	531.705653	9.329703
7.942516	527.825430	9.334720
7.551265	536.946597	9.339738
7.732222	534.285048	9.344755
8.146615	552.601106	9.349773
8.124957	549.863468	9.354791
7.959054	540.878691	9.359808
7.696163	533.441370	9.364826
7.584184	535.544338	9.369843
7.843918	541.708500	9.374861
7.672614	536.124189	9.379879
7.793721	537.412631	9.384896
7.308721	559.437225	9.389914
7.814224	550.352680	9.394931
7.982462	560.266784	9.399949
8.071855	566.242248	9.404967
8.342089	566.062985	9.409984
8.247039	561.009506	9.415002
8.063875	541.189155	9.420019
7.522310	537.633539	9.425037
7.407652	540.606379	9.430055
8.111051	547.996002	9.435072
7.856227	561.179549	9.440090
7.742075	561.472570	9.445107
7.939005	568.089829	9.450125
7.661349	573.140513	9.455143
8.025187	573.032752	9.460160
7.916245	577.228586	9.465178
7.932291	561.687139	9.470195
8.042858	559.813960	9.475213
8.149313	561.619755	9.480231
8.282237	565.094086	9.485248
7.973399	566.368494	9.490266
7.721877	566.259489	9.495283
8.221743	562.529447	9.500301
7.976305	564.362216	9.505319
8.380005	559.340117	9.510336
7.886913	569.390704	9.515354
7.722173	552.903873	9.520371
8.007199	566.344856	9.525389
7.751689	571.001937	9.530407
8.097552	561.777691	9.535424
8.062809	566.112407	9.540442
8.020677	564.422770	9.545459
7.958902	555.187688	9.550477
7.996600	562.322813	9.555495
7.906507	560.918068	9.560512
7.879872	561.576297	9.565530
7.941582	563.578662	9.570547
8.121411	562.307358	9.575565
7.658934	557.540101	9.580583
8.052875	573.043817	9.585600
8.157909	591.352492	9.590618
8.104231	590.256851	9.595635
8.341214	592.628989	9.600653
8.415737	588.927644	9.605671
8.486759	580.329568	9.610688
8.286968	582.511450	9.615706
8.106588	563.893481	9.620723
8.027302	561.420287	9.625741
8.200674	565.787465	9.630759
8.334163	561.070919	9.635776
8.057599	572.756012	9.640794
8.283443	577.974683	9.645811
8.452767	585.287419	9.650829
8.268949	576.980150	9.655847
8.322310	560.382201	9.660864
8.235399	557.664814	9.665882
8.282495	558.531881	9.670899
7.968282	554.878185	9.675917
8.013719	572.288893	9.680935
8.696500	589.238988	9.685952
8.478123	576.534781	9.690970
8.538027	566.923267	9.695987
8.324820	550.530876	9.701005
8.169348	564.642594	9.706023
8.017441	558.047454	9.711040
8.320892	556.965902	9.716058
8.112513	576.624203	9.721075
8.149132	580.292228	9.726093
8.217908	595.502394	9.731111
8.388492	585.600906	9.736128
8.145258	587.919501	9.741146
8.534394	585.195519	9.746163
8.532863	591.821440	9.751181
8.430610	591.622958	9.756199
8.476429	591.873940	9.761216
8.627410	599.555641	9.766234
8.233500	589.426387	9.771251
8.482049	587.028814	9.776269
8.096747	596.381890	9.781287
8.304441	590.837550	9.786304
8.132493	589.415650	9.791322
8.403014	592.629423	9.796339
8.640029	592.403498	9.801357
8.468260	593.580610	9.806375
8.600562	595.763994	9.811392
8.426457	601.757320	9.816410
8.617169	600.897372	9.821427
8.822120	592.493436	9.826445
8.414021	591.744852	9.831463
8.659463	595.969995	9.836480
8.708383	594.072180	9.841498
8.379133	583.866281	9.846515
8.107560	580.654897	9.851533
8.227899	599.050804	9.856551
8.281354	588.689016	9.861568
8.473174	582.642813	9.866586
8.721357	592.598223	9.871603
8.937795	598.040098	9.876621
8.712432	605.486306	9.881639
8.581590	594.077150	9.886656
8.380928	607.463760	9.891674
8.424248	598.427377	9.896691
8.750382	591.357223	9.901709
8.594612	600.180987	9.906727
8.560116	593.616780	9.911744
8.530367	600.269817	9.916762
8.562327	602.067088	9.921779
8.749677	588.445545	9.926797
8.500487	593.729498	9.931815
8.859056	592.041808	9.936832
8.897593	596.310661	9.941850
8.510313	596.861495	9.946867
8.892709	591.597064	9.951885
8.445835	596.028575	9.956903
9.037584	596.256868	9.961920
9.098925	596.266910	9.966938
8.749210	583.584051	9.971955
8.741632	565.572070	9.976973
8.826246	571.455027	9.981991
8.745623	560.803473	9.987008
8.641989	570.349048	9.992026
8.261509	560.279789	9.997043
8.899243	565.447769	10.002061
8.594616	587.126020	10.007079
8.712713	593.294957	10.012096
8.597935	602.188700	10.017114
8.826720	593.386355	10.022131
8.596816	595.277772	10.027149
8.223435	600.279753	10.032167
8.595881	596.058631	10.037184
8.883872	590.660236	10.042202
8.688839	603.170378	10.047219
9.013961	594.125716	10.052237
8.845065	597.965761	10.057255
8.957857	599.417975	10.062272
8.656703	594.470262	10.067290
9.045152	595.021768	10.072307
8.934442	588.822917	10.077325
8.922389	600.549066	10.082343
8.691029	599.862744	10.087360
8.910610	595.758268	10.092378
8.902335	599.528805	10.097395
9.018343	590.688053	10.102413
8.734889	599.100114	10.107431
9.223387	597.930440	10.112448
8.995132	599.553491	10.117466
8.796716	600.927523	10.122483
8.936486	607.103112	10.127501
8.701314	602.625542	10.132519
8.820050	605.913267	10.137536
8.890738	597.501052	10.142554
8.972129	601.889180	10.147571
9.277732	601.374750	10.152589
8.858275	601.252808	10.157607
8.894405	598.646133	10.162624
9.100285	599.677251	10.167642
8.631437	604.877707	10.172659
8.816621	600.916122	10.177677
8.815818	604.206517	10.182695
8.735000	603.096866	10.187712
8.636358	604.123887	10.192730
8.572972	601.474246	10.197747
8.988409	611.833834	10.202765
8.971024	625.262744	10.207783
8.995141	630.335321	10.212800
8.953929	630.439505	10.217818
8.847405	637.987893	10.222835
9.022612	626.183371	10.227853
9.028217	632.838441	10.232871
8.832830	630.897814	10.237888
9.320355	630.566041	10.242906
8.861386	631.957042	10.247923
9.211358	626.075960	10.252941
9.117899	641.251622	10.257959
8.864698	632.522966	10.262976
9.214424	632.117560	10.267994
8.844136	636.575965	10.273011
8.996573	627.384497	10.278029
8.897667	632.318401	10.283047
8.722895	624.653071	10.288064
9.131138	630.926921	10.293082
8.988189	650.296742	10.298099
9.402567	648.551186	10.303117
9.346592	656.355762	10.308135
9.056908	644.871107	10.313152
9.371248	641.322152	10.318170
9.182809	651.813061	10.323187
9.541112	640.007735	10.328205
9.029122	638.188821	10.333223
9.369838	637.723494	10.338240
9.269966	631.047664	10.343258
9.335776	627.475697	10.348275
9.391051	625.197913	10.353293
9.037283	634.279665	10.358311
9.242693	627.415104	10.363328
9.490705	636.674749	10.368346
9.485094	645.017796	10.373363
9.602377	633.289392	10.378381
9.103417	633.092234	10.383399
8.804816	628.102357	10.388416
9.403768	645.798633	10.393434
9.298725	649.187986	10.398451
9.516905	654.223318	10.403469
9.443896	650.530248	10.408487
9.480611	640.659946	10.413504
9.290122	637.674872	10.418522
9.352799	642.995383	10.423539
9.309912	642.449098	10.428557
9.330838	631.949173	10.433575
9.361673	654.584503	10.438592
9.622050	652.125123	10.443610
9.496836	654.508825	10.448627
9.303736	641.450401	10.453645
9.590623	637.406418	10.458663
9.296996	652.302265	10.463680
9.382872	643.518635	10.468698
9.424534	654.213947	10.473715
9.352820	662.587633	10.478733
9.539496	659.555453	10.483751
9.270757	659.381192	10.488768
9.500421	652.755896	10.493786
9.535959	666.990595	10.498803
9.659144	651.421277	10.503821
9.697015	658.294623	10.508839
9.738279	660.983022	10.513856
9.813244	657.251668	10.518874
9.226499	644.975703	10.523891
9.420163	642.195897	10.528909
9.666550	652.962026	10.533927
9.400358	658.176380	10.538944
9.636399	654.644324	10.543962
9.634893	657.406336	10.548979
9.730294	655.872644	10.553997
9.708692	661.660632	10.559015
9.569549	660.594492	10.564032
9.967332	649.239680	10.569050
9.640078	646.846114	10.574067
9.443601	639.540648	10.579085
9.624886	646.589441	10.584103
9.528735	657.231597	10.589120
9.907293	656.829684	10.594138
9.634261	654.229906	10.599155
9.712418	653.634445	10.604173
9.580146	647.579289	10.609191
9.271607	658.283778	10.614208
9.984053	647.513830	10.619226
9.518691	662.414110	10.624243
9.513512	657.668138	10.629261
9.874548	664.042726	10.634279
9.277790	653.545863	10.639296
9.641990	657.677937	10.644314
9.427253	656.675493	10.649331
9.609286	658.444179	10.654349
9.529892	660.279777	10.659367
9.265781	652.775675	10.664384
9.485818	661.692745	10.669402
9.293705	674.561297	10.674419
9.630065	678.146839	10.679437
9.944415	688.933233	10.684455
9.682425	694.795289	10.689472
10.025808	690.929328	10.694490
9.844857	694.217882	10.699507
10.016932	690.031096	10.704525
9.995937	694.578912	10.709543
9.785002	702.483971	10.714560
9.730226	689.021521	10.719578
9.538604	692.535056	10.724595
10.064186	698.636756	10.729613
9.877965	693.967599	10.734631
10.049499	703.035236	10.739648
10.203090	691.140155	10.744666
10.057435	696.434162	10.749683
10.023019	690.387587	10.754701
10.235348	687.708219	10.759719
9.984618	690.539063	10.764736
10.301013	688.024342	10.769754
9.990500	685.775232	10.774771
10.122806	681.576531	10.779789
9.972716	660.427599	10.784807
9.852618	668.770326	10.789824
10.085658	666.279253	10.794842
9.750562	667.476920	10.799859
9.831638	668.197431	10.804877
10.340597	679.396447	10.809895
9.744415	690.026943	10.814912
10.247242	687.240026	10.819930
9.875893	694.577978	10.824947
9.797663	682.213448	10.829965
9.988159	686.147929	10.834983
9.610896	693.838414	10.840000
10.207233	681.700744	10.845018
9.864131	683.866609	10.850035
9.965339	683.421652	10.855053
10.096874	688.681566	10.860071
9.786960	697.323441	10.865088
9.917299	692.278656	10.870106
9.865885	697.000398	10.875123
10.166283	703.098446	10.880141
10.052070	696.147420	10.885159
10.131073	703.835580	10.890176
10.255293	707.106278	10.895194
9.951083	715.714150	10.900211
10.195001	725.120974	10.905229
10.386995	711.798734	10.910247
10.391664	718.277628	10.915264
10.497865	710.904292	10.920282
10.430724	700.233088	10.925299
10.234349	702.019168	10.930317
10.407630	675.916956	10.935335
10.463996	692.074884	10.940352
10.041002	684.234106	10.945370
10.370613	687.524329	10.950387
10.160369	690.873634	10.955405
10.189041	682.348259	10.960423
10.189862	694.976625	10.965440
10.479469	683.625528	10.970458
10.763203	693.290685	10.975475
10.534772	689.757192	10.980493
10.674486	695.701147	10.985511
10.450463	703.026911	10.990528
10.516673	685.774967	10.995546
10.731405	685.833620	11.000563
10.649629	685.537460	11.005581
10.462724	692.745269	11.010599
10.408176	688.502708	11.015616
10.774885	685.965483	11.020634
10.554836	688.226713	11.025651
10.245702	683.886162	11.030669
10.454191	687.344858	11.035687
10.227656	695.925291	11.040704
10.324083	695.389398	11.045722
10.269000	680.160576	11.050739
10.268600	695.275215	11.055757
10.407069	687.798914	11.060775
10.262591	695.454396	11.065792
10.421469	687.666861	11.070810
10.251892	688.389904	11.075827
9.895348	692.429538	11.080845
10.322545	698.686891	11.085863
10.319844	712.507122	11.090880
10.477961	723.728443	11.095898
10.478630	718.091771	11.100915
10.746846	724.485297	11.105933
10.737317	712.298725	11.110951
10.483794	731.476734	11.115968
10.467832	717.876737	11.120986
10.702710	725.037157	11.126003
10.572094	734.329639	11.131021
10.745407	720.614444	11.136039
10.373186	717.474812	11.141056
10.385107	719.342537	11.146074
10.742792	721.232530	11.151091
10.421961	722.816006	11.156109
10.788113	722.398824	11.161127
10.718018	731.827337	11.166144
10.323405	717.654644	11.171162
10.444330	718.583506	11.176179
10.243400	714.835624	11.181197
10.514862	710.888265	11.186215
10.528559	719.313189	11.191232
10.495538	717.530300	11.196250
10.627167	727.750556	11.201267
10.460876	748.686481	11.206285
10.606243	752.122969	11.211303
10.856552	758.223427	11.216320
10.701597	754.011648	11.221338
10.769002	759.502272	11.226355
10.614581	758.307954	11.231373
10.772642	753.351861	11.236391
10.982904	759.226680	11.241408
11.007134	753.924658	11.246426
10.917341	748.556091	11.251443
10.729672	757.559232	11.256461
10.893635	754.503237	11.261479
10.841989	755.111091	11.266496
10.637366	754.406161	11.271514
10.949770	749.650483	11.276531
10.845993	753.671504	11.281549
10.775331	753.117610	11.286567
10.906810	756.232401	11.291584
11.059720	752.066881	11.296602
11.153346	745.252667	11.301619
10.743086	755.422917	11.306637
11.194531	749.817095	11.311655
11.179743	742.410239	11.316672
11.081301	755.247993	11.321690
11.149466	757.037909	11.326707
11.075892	764.401778	11.331725
11.206840	746.639467	11.336743
11.308172	755.253037	11.341760
11.162839	749.216933	11.346778
11.060796	727.651314	11.351795
10.751989	718.350747	11.356813
11.051340	737.835222	11.361831
11.034673	743.478730	11.366848
10.944776	750.704753	11.371866
11.421583	752.589196	11.376883
11.114517	753.086204	11.381901
11.177414	742.129279	11.386919
11.084494	733.209073	11.391936
10.603917	739.589992	11.396954
10.848336	744.093479	11.401971
10.798515	756.922790	11.406989
10.980749	744.679243	11.412007
11.011222	748.731179	11.417024
11.006718	756.991824	11.422042
11.043824	750.036581	11.427059
11.210023	756.349381	11.432077
11.048220	751.032499	11.437095
10.914048	751.681181	11.442112
11.019932	760.094012	11.447130
11.220861	754.919414	11.452147
11.074872	767.733164	11.457165
11.333866	776.301742	11.462183
11.571749	776.360105	11.467200
11.273985	764.674740	11.472218
11.225834	761.581431	11.477235
10.892313	764.853534	11.482253
11.291195	777.027096	11.487271
11.312879	776.858282	11.492288
11.204197	788.948194	11.497306
11.570965	783.136709	11.502323
11.226452	780.421981	11.507341
11.043636	786.854001	11.512359
11.239939	791.239098	11.517376
11.050094	788.232630	11.522394
11.675000	792.444004	11.527411
11.184862	791.945398	11.532429
11.250712	784.168889	11.537447
11.392686	785.412756	11.542464
11.090756	788.968987	11.547482
11.505295	791.133024	11.552499
11.467888	788.341457	11.557517
11.165118	790.618762	11.562535
11.352652	789.158773	11.567552
11.198152	784.574489	11.572570
11.411622	781.763427	11.577587
11.313588	783.777707	11.582605
11.416895	782.704480	11.587623
11.728445	785.939844	11.592640
11.337669	781.893478	11.597658
11.527764	785.481613	11.602675
11.389594	796.970935	11.607693
11.635509	806.541642	11.612711
11.868959	803.114308	11.617728
11.568614	799.165555	11.622746
11.544298	787.062472	11.627763
11.547770	786.745107	11.632781
11.636131	782.806791	11.637799
11.614391	782.105827	11.642816
11.499077	797.230145	11.647834
12.004947	789.202433	11.652851
11.770466	793.557295	11.657869
12.007544	787.502338	11.662887
12.258069	790.089969	11.667904
11.646603	790.066548	11.672922
11.966550	779.305602	11.677939
11.744054	787.503940	11.682957
11.799361	779.439037	11.687975
11.254099	782.106082	11.692992
11.454589	789.074993	11.698010
11.830860	781.302197	11.703027
11.602006	781.277620	11.708045
11.992018	783.296513	11.713063
11.864596	785.196374	11.718080
11.615732	784.240121	11.723098
11.751423	773.321118	11.728115
11.964777	784.397910	11.733133
11.475406	784.011769	11.738151
11.868963	780.658316	11.743168
11.586186	786.762813	11.748186
11.892620	775.110848	11.753203
11.905752	783.435118	11.758221
11.750209	779.154535	11.763239
11.683771	782.085581	11.768256
11.683456	798.667550	11.773274
12.060884	808.593234	11.778291
11.851322	810.905104	11.783309
12.054662	823.442956	11.788327
12.258483	802.727326	11.793344
11.808563	795.817278	11.798362
12.090657	783.098922	11.803379
11.659766	792.956882	11.808397
11.860170	801.652886	11.813415
12.154869	803.635598	11.818432
12.150792	804.553671	11.823450
11.573363	794.094059	11.828467
11.993117	797.285919	11.833485
12.157899	813.399644	11.838503
12.448020	820.406874	11.843520
11.952212	809.682174	11.848538
12.011818	794.466137	11.853555
11.827625	802.346346	11.858573
12.131039	812.808670	11.863591
12.297930	827.639057	11.868608
12.184626	821.860205	11.873626
12.126846	803.381481	11.878643
12.130699	803.443561	11.883661
11.912215	810.346039	11.888679
11.989138	809.069316	11.893696
11.968450	822.082036	11.898714
11.822870	810.677326	11.903731
11.878424	815.632165	11.908749
11.918087	827.124737	11.913767
12.171740	814.768920	11.918784
11.995669	817.995671	11.923802
12.190679	814.137321	11.928819
12.191985	816.145391	11.933837
12.240732	818.021202	11.938855
12.291386	822.108002	11.943872
12.160743	819.959790	11.948890
12.199998	820.272687	11.953907
12.224859	818.797901	11.958925
12.192348	811.776210	11.963943
12.144398	815.075047	11.968960
12.113253	833.725833	11.973978
12.262195	849.285159	11.978995
12.663500	839.617338	11.984013
12.472713	838.672723	11.989031
12.611703	822.119171	11.994048
12.299620	824.473609	11.999066
12.326258	817.436609	12.004083
12.432536	821.108707	12.009101
12.437490	821.735930	12.014119
12.430902	811.789623	12.019136
12.308883	815.388112	12.024154
12.443672	828.156992	12.029171
12.216577	837.902497	12.034189
12.217548	842.649859	12.039207
12.644595	838.939684	12.044224
12.412324	846.642454	12.049242
12.624662	834.386371	12.054259
12.649411	840.416345	12.059277
12.506258	849.568065	12.064295
12.733348	849.082180	12.069312
12.596095	846.744910	12.074330
12.577777	842.134122	12.079347
12.654044	843.766415	12.084365
12.561294	843.833468	12.089383
12.726930	835.375875	12.094400
12.246970	838.265175	12.099418
12.192003	844.541803	12.104435
12.409725	846.767965	12.109453
12.248621	845.492467	12.114471
12.837568	842.970776	12.119488
12.730793	848.662314	12.124506
12.912313	840.372158	12.129523
12.653287	845.562554	12.134541
12.148318	843.616080	12.139559
12.864970	845.941505	12.144576
12.805154	848.404166	12.149594
12.746828	839.998617	12.154611
12.393727	842.001994	12.159629
12.142528	848.727632	12.164647
12.324989	842.201013	12.169664
12.200407	860.842895	12.174682
12.645795	862.506582	12.179699
12.959010	869.919439	12.184717
12.844517	882.522959	12.189735
13.171686	876.127868	12.194752
13.036735	889.434355	12.199770
13.019287	871.707497	12.204787
13.128467	862.693517	12.209805
12.664718	861.426403	12.214823
12.781848	850.252164	12.219840
12.561865	870.265693	12.224858
13.041990	883.392375	12.229875
13.165002	877.973564	12.234893
12.889572	886.335044	12.239911
13.190629	873.585916	12.244928
12.740395	871.613053	12.249946
12.953348	875.007669	12.254963
12.710203	873.037126	12.259981
12.753775	887.536432	12.264999
12.776460	880.749653	12.270016
12.761588	880.165258	12.275034
12.786275	881.823812	12.280051
12.921741	877.624535	12.285069
12.907463	879.010420	12.290087
13.114857	881.263493	12.295104
12.844131	886.323562	12.300122
13.203220	882.267167	12.305139
13.082305	871.755136	12.310157
13.127442	881.013090	12.315175
13.135085	871.506494	12.320192
13.126183	878.140451	12.325210
12.770636	876.833371	12.330227
13.126787	870.531903	12.335245
12.903429	888.962627	12.340263
13.186555	870.537210	12.345280
12.987874	881.871268	12.350298
12.992487	893.855498	12.355315
13.069292	904.877432	12.360333
13.136094	913.196427	12.365351
13.147180	910.272405	12.370368
13.356107	912.753565	12.375386
13.524120	909.623251	12.380403
13.748581	914.078914	12.385421
13.025960	907.082483	12.390439
13.515397	892.390816	12.395456
13.513564	898.517729	12.400474
13.459088	890.975254	12.405491
13.423142	880.230653	12.410509
13.189957	877.836433	12.415527
13.579473	878.061805	12.420544
13.194107	890.683416	12.425562
13.463792	879.231544	12.430579
13.603393	867.172511	12.435597
13.400578	877.755712	12.440615
13.366446	877.335916	12.445632
13.417089	871.873582	12.450650
13.053119	874.718880	12.455667
13.417671	878.647029	12.460685
13.171029	895.047854	12.465703
13.161104	904.824759	12.470720
13.113207	911.231733	12.475738
13.226213	907.899908	12.480755
13.661155	905.304501	12.485773
13.229892	911.574966	12.490791
13.689939	903.787056	12.495808
13.175196	909.629238	12.500826
13.605902	905.481454	12.505843
13.706381	905.505487	12.510861
13.402372	905.509102	12.515879
13.703413	909.047793	12.520896
13.608629	909.325803	12.525914
13.464454	908.865963	12.530931
13.562236	912.338318	12.535949
13.532925	914.817985	12.540967
13.388986	904.433754	12.545984
13.534537	908.232040	12.551002
13.673098	903.807845	12.556019
13.607624	899.855999	12.561037
13.539136	907.805287	12.566055
13.811318	920.312526	12.571072
13.775918	923.088859	12.576090
13.310530	934.188391	12.581107
13.977075	936.866601	12.586125
13.908998	943.235593	12.591143
13.764253	933.753799	12.596160
13.985139	935.972364	12.601178
13.858496	938.603185	12.606195
13.923634	922.977462	12.611213
13.699003	925.159567	12.616231
13.917302	929.704834	12.621248
14.184311	918.801777	12.626266
13.599154	913.982875	12.631283
14.170981	911.577389	12.636301
13.690901	914.961977	12.641319
13.735236	916.187379	12.646336
14.105668	927.153227	12.651354
13.869445	930.954897	12.656371
14.205459	924.554778	12.661389
13.773168	919.943622	12.666407
13.962635	935.010913	12.671424
14.162409	933.504003	12.676442
14.065100	928.040559	12.681459
14.141987	899.715844	12.686477
13.813653	906.919614	12.691495
13.597633	904.663879	12.696512
14.141328	927.664268	12.701530
13.845970	940.387545	12.706547
14.377397	932.550007	12.711565
14.438854	943.229250	12.716583
14.119769	930.678823	12.721600
14.088112	922.681000	12.726618
13.931204	939.917762	12.731635
14.246558	938.355101	12.736653
14.172875	941.419260	12.741671
14.219269	938.568910	12.746688
14.364641	938.175685	12.751706
14.124265	934.557897	12.756723
14.357343	940.626637	12.761741
14.486666	923.734040	12.766759
14.248121	915.109091	12.771776
14.102398	912.528343	12.776794
13.994963	915.074094	12.781811
14.672278	919.932308	12.786829
13.984498	923.598917	12.791847
13.962991	925.094660	12.796864
14.600434	939.983450	12.801882
14.368002	941.547191	12.806899
14.561243	932.720817	12.811917
14.055140	924.511411	12.816935
14.046023	923.498127	12.821952
14.519142	933.854089	12.826970
14.228161	939.945438	12.831987
14.633771	939.703993	12.837005
14.109020	939.022144	12.842023
14.427534	934.903560	12.847040
14.398523	941.073571	12.852058
14.095826	948.016432	12.857075
14.256162	941.531622	12.862093
14.244163	935.956809	12.867111
14.216999	942.198953	12.872128
14.411943	946.735494	12.877146
14.697923	947.586253	12.882163
14.840833	935.618742	12.887181
14.276288	947.078782	12.892199
14.506189	945.844036	12.897216
14.605529	936.752906	12.902234
14.489917	942.119970	12.907251
14.427486	945.036998	12.912269
14.092758	944.068970	12.917287
14.489518	942.569596	12.922304
14.913305	956.244229	12.927322
14.988185	960.296740	12.932339
14.623373	944.641407	12.937357
14.397485	942.350295	12.942375
14.565906	937.964844	12.947392
14.898052	957.198112	12.952410
14.545711	957.725062	12.957427
14.738104	954.646605	12.962445
14.620338	964.235115	12.967463
14.635435	972.133588	12.972480
14.690432	975.701227	12.977498
14.727499	973.909459	12.982515
14.680457	973.916583	12.987533
14.769349	971.726485	12.992551
14.550896	973.476096	12.997568
14.850413	969.122469	13.002586
14.651509	962.615644	13.007603
14.674175	971.164805	13.012621
14.735221	961.739464	13.017639
14.301883	969.555506	13.022656
14.785198	961.912921	13.027674
14.334684	976.619318	13.032691
14.694628	986.259046	13.037709
15.244626	996.524371	13.042727
15.108149	1009.270999	13.047744
15.605256	1004.013811	13.052762
15.231858	978.725210	13.057779
15.424919	962.518838	13.062797
15.227030	960.531735	13.067815
15.323125	964.649235	13.072832
15.288039	958.340079	13.077850
14.846439	966.235438	13.082867
15.059637	962.566944	13.087885
15.218258	965.696967	13.092903
14.812965	971.516717	13.097920
15.258523	958.583756	13.102938
15.004804	965.293721	13.107955
14.789839	961.438264	13.112973
14.829255	957.363134	13.117991
14.818583	960.619610	13.123008
15.211634	973.670634	13.128026
14.953057	995.713860	13.133043
15.619816	990.423467	13.138061
15.081902	986.721870	13.143079
15.172862	988.415523	13.148096
15.441953	988.709261	13.153114
15.356599	985.859854	13.158131
15.231816	970.363559	13.163149
15.350712	972.141163	13.168167
15.547644	972.391734	13.173184
15.414453	967.084606	13.178202
15.621446	962.614417	13.183219
15.103439	973.712455	13.188237
15.463798	961.678996	13.193255
15.049602	962.174065	13.198272
15.364002	958.549835	13.203290
15.213754	972.709284	13.208307
15.303120	977.455042	13.213325
15.561359	981.118943	13.218343
15.507498	1001.981476	13.223360
15.613619	990.270004	13.228378
15.364520	982.326265	13.233395
15.594442	990.309249	13.238413
15.716636	979.755707	13.243431
15.553393	969.917520	13.248448
15.466670	968.503322	13.253466
15.295437	969.495931	13.258483
15.086964	981.951716	13.263501
15.802754	989.746375	13.268519
15.478924	1001.281157	13.273536
15.407952	998.643531	13.278554
15.513068	998.339644	13.283571
15.496033	995.611987	13.288589
15.461898	1003.167462	13.293607
15.311818	1002.722769	13.298624
15.701857	1001.843376	13.303642
15.629344	998.033217	13.308659
15.575813	991.927880	13.313677
15.587670	984.965691	13.318695
15.593441	993.283025	13.323712
15.674603	993.876376	13.328730
15.624315	1002.310474	13.333747
15.640615	989.891464	13.338765
15.821741	990.175360	13.343783
16.041542	1014.451117	13.348800
15.761802	997.766722	13.353818
15.814877	995.316421	13.358835
16.221917	999.931238	13.363853
15.610015	999.909855	13.368871
15.860727	993.612806	13.373888
15.890231	989.886932	13.378906
15.678529	991.927935	13.383923
15.958726	1009.835279	13.388941
16.106507	1012.491928	13.393959
15.886137	1021.606143	13.398976
15.899127	1013.565054	13.403994
15.996906	1018.957044	13.409011
15.662533	1014.577273	13.414029
16.063974	1019.702059	13.419047
15.895737	1020.937867	13.424064
16.129823	1009.857528	13.429082
16.142622	1023.790426	13.434099
16.084769	1018.174359	13.439117
16.154480	1014.435129	13.444135
16.107864	1015.391359	13.449152
16.308511	1025.959425	13.454170
16.296165	1027.287525	13.459187
16.228180	1031.282612	13.464205
16.105075	1023.129807	13.469223
15.941969	1028.708302	13.474240
16.378153	1011.806921	13.479258
16.099512	1028.532464	13.484275
16.134134	1024.706132	13.489293
16.172074	1024.462186	13.494311
15.930484	1021.721710	13.499328
15.906993	1024.312237	13.504346
16.250415	1017.853375	13.509363
16.340830	1021.329730	13.514381
16.308599	1014.202393	13.519399
15.903668	1021.700778	13.524416
16.113899	1017.747734	13.529434
16.337901	1017.800131	13.534451
16.278981	1024.644393	13.539469
16.373275	1026.707562	13.544487
16.285684	1025.650576	13.549504
16.433960	1017.034348	13.554522
16.582358	1020.031828	13.559539
16.355736	1022.992986	13.564557
16.643933	1022.721379	13.569575
16.317120	1024.105488	13.574592
16.490078	1022.416404	13.579610
16.008855	1026.246856	13.584627
16.387531	1045.455994	13.589645
16.808603	1045.713151	13.594663
16.635802	1047.804410	13.599680
16.629854	1054.745422	13.604698
16.667296	1047.601415	13.609715
16.451400	1057.271583	13.614733
17.119448	1055.138715	13.619751
16.634660	1046.830442	13.624768
16.742459	1021.097930	13.629786
16.745136	1023.898682	13.634803
16.729920	1020.645937	13.639821
16.622245	1012.391767	13.644839
16.620687	1024.160986	13.649856
16.738485	1021.863736	13.654874
16.827624	1020.576705	13.659891
16.403586	1021.946600	13.664909
16.538403	1031.489783	13.669927
16.646661	1053.531794	13.674944
16.677357	1047.043211	13.679962
16.845977	1043.955287	13.684979
16.656846	1048.148780	13.689997
17.135528	1038.925486	13.695015
17.018921	1048.350082	13.700032
17.010088	1044.355751	13.705050
17.190762	1046.601068	13.710067
16.948877	1049.726958	13.715085
17.347033	1048.035225	13.720103
16.888089	1035.645269	13.725120
17.125140	1029.322122	13.730138
16.705651	1025.074548	13.735155
16.709268	1036.655524	13.740173
17.129472	1043.649582	13.745191
17.109390	1050.957880	13.750208
16.950217	1040.372151	13.755226
17.049684	1043.845831	13.760243
16.952858	1052.317977	13.765261
17.120914	1050.084839	13.770279
16.733402	1049.045232	13.775296
17.012317	1042.431300	13.780314
17.113011	1051.698660	13.785331
16.785116	1054.719900	13.790349
16.864892	1045.617773	13.795367
16.939961	1054.487424	13.800384
17.117340	1058.219456	13.805402
17.365718	1044.301001	13.810419
17.036530	1054.063940	13.815437
17.054078	1051.233700	13.820455
17.293009	1055.775194	13.825472
17.060258	1053.672203	13.830490
17.374731	1056.640615	13.835507
17.000470	1080.484943	13.840525
17.256759	1069.567808	13.845543
17.113469	1082.430581	13.850560
17.089648	1079.780409	13.855578
17.518417	1078.262731	13.860595
17.426495	1081.216949	13.865613
17.632354	1072.728946	13.870631
17.591697	1075.815220	13.875648
17.557136	1078.595379	13.880666
17.712272	1077.124586	13.885683
17.879493	1076.158862	13.890701
17.425044	1057.593163	13.895719
17.624033	1055.367894	13.900736
17.242808	1050.541950	13.905754
17.492688	1045.190653	13.910771
17.116283	1057.295579	13.915789
17.363386	1058.703550	13.920807
17.410878	1066.308529	13.925824
17.400050	1071.395698	13.930842
17.830916	1066.063241	13.935859
17.457540	1078.362557	13.940877
17.791263	1064.920092	13.945895
17.769351	1075.640789	13.950912
17.516349	1076.476085	13.955930
17.614691	1072.406915	13.960947
17.359723	1086.745613	13.965965
17.774467	1074.589680	13.970983
17.888583	1082.018285	13.976000
17.631011	1087.226236	13.981018
17.747749	1077.606964	13.986035
17.727812	1086.928177	13.991053
17.866895	1081.081846	13.996071
17.646726	1086.380450	14.001088
17.664780	1070.028936	14.006106
17.965660	1079.563154	14.011123
17.853353	1082.153044	14.016141
18.081773	1077.110397	14.021159
18.046286	1078.103369	14.026176
17.664231	1088.884105	14.031194
17.729746	1084.488095	14.036211
17.480427	1081.019386	14.041229
17.566417	1097.896822	14.046247
17.564426	1114.786483	14.051264
17.947905	1113.969192	14.056282
17.915128	1104.161283	14.061299
17.968805	1116.107245	14.066317
18.258253	1099.595016	14.071335
18.164219	1109.893835	14.076352
17.852932	1109.751809	14.081370
18.251785	1109.558330	14.086387
18.246680	1112.031658	14.091405
18.588743	1099.349963	14.096423
18.159398	1108.116168	14.101440
18.170711	1108.674635	14.106458
18.398412	1108.229979	14.111475
18.484429	1109.123702	14.116493
18.215959	1110.434774	14.121511
18.220072	1113.929771	14.126528
18.075604	1109.444119	14.131546
18.381476	1098.979369	14.136563
18.313914	1106.479013	14.141581
18.471085	1107.665668	14.146599
18.451004	1109.232844	14.151616
18.315664	1116.107123	14.156634
18.450154	1105.102262	14.161651
18.111920	1109.435417	14.166669
18.532537	1100.820502	14.171687
18.299843	1099.585576	14.176704
18.232611	1102.758143	14.181722
18.042201	1108.567558	14.186739
18.028150	1112.159654	14.191757
18.293218	1100.698935	14.196775
18.115107	1104.455986	14.201792
18.208902	1119.075535	14.206810
18.702596	1124.422868	14.211827
18.245238	1136.729050	14.216845
18.484728	1123.205291	14.221863
18.521716	1130.781727	14.226880
18.647997	1122.967877	14.231898
18.492678	1129.181712	14.236915
18.649302	1130.877498	14.241933
18.746412	1123.574761	14.246951
18.726316	1133.455460	14.251968
18.630385	1127.176389	14.256986
19.344878	1123.566970	14.262003
18.627536	1138.511791	14.267021
18.679495	1133.290872	14.272039
19.071057	1130.433723	14.277056
18.942253	1132.188191	14.282074
19.039361	1127.757017	14.287091
18.711567	1116.589334	14.292109
18.945194	1122.473415	14.297127
19.164960	1110.137542	14.302144
18.780463	1102.609456	14.307162
18.958190	1089.872306	14.312179
18.595231	1102.966346	14.317197
18.883913	1111.851050	14.322215
18.793702	1111.892487	14.327232
18.804685	1124.432121	14.332250
19.041455	1122.365148	14.337267
18.844015	1122.880232	14.342285
18.780142	1118.731615	14.347303
19.160142	1119.362492	14.352320
18.822793	1133.514094	14.357338
18.886780	1123.461022	14.362355
18.757604	1126.098594	14.367373
18.819796	1128.651329	14.372391
19.043858	1121.285053	14.377408
18.751407	1131.186441	14.382426
18.951577	1120.477769	14.387443
19.307717	1138.765982	14.392461
19.277823	1139.895035	14.397479
19.131903	1136.330848	14.402496
19.378979	1146.712967	14.407514
19.404547	1130.137318	14.412531
18.998905	1135.512712	14.417549
19.212030	1142.805665	14.422567
19.675253	1150.955999	14.427584
19.630272	1147.519972	14.432602
19.638071	1131.081512	14.437619
19.657756	1125.971054	14.442637
19.422378	1122.421683	14.447655
19.430303	1125.880620	14.452672
19.328792	1125.504650	14.457690
19.468846	1119.144381	14.462707
19.372237	1127.603933	14.467725
19.370963	1128.420382	14.472743
19.356866	1125.065858	14.477760
19.164748	1128.041007	14.482778
19.329736	1127.270525	14.487795
19.592375	1136.712295	14.492813
19.413177	1147.854743	14.497831
19.450504	1151.728489	14.502848
19.392090	1165.137102	14.507866
19.410163	1165.977514	14.512883
19.184118	1159.448329	14.517901
19.387981	1155.264029	14.522919
19.343958	1152.927022	14.527936
19.179778	1161.085980	14.532954
19.547788	1166.810035	14.537971
19.248280	1169.544714	14.542989
19.431081	1179.096184	14.548007
19.753521	1184.029781	14.553024
19.941132	1183.423657	14.558042
20.005314	1187.426425	14.563059
20.225579	1188.366819	14.568077
19.697608	1189.029942	14.573095
20.059134	1180.664524	14.578112
19.956829	1185.635386	14.583130
19.786360	1175.578192	14.588147
19.680038	1177.069894	14.593165
19.848605	1179.488097	14.598183
19.937070	1179.863323	14.603200
20.154160	1184.974992	14.608218
20.476444	1176.118057	14.613235
20.127694	1156.517048	14.618253
20.118049	1154.070415	14.623271
20.663432	1149.989796	14.628288
19.916067	1154.612358	14.633306
20.276214	1149.293158	14.638323
20.218344	1146.569874	14.643341
20.432044	1155.863859	14.648359
20.637557	1143.122064	14.653376
20.334647	1153.878322	14.658394
20.394661	1148.251745	14.663411
20.097801	1145.377884	14.668429
19.983736	1144.889429	14.673447
20.172628	1143.935466	14.678464
20.142055	1148.007457	14.683482
20.324729	1139.255942	14.688499
20.471096	1144.697802	14.693517
20.180604	1155.454367	14.698535
20.127736	1147.703632	14.703552
19.942885	1153.378683	14.708570
20.180124	1145.502748	14.713587
20.181790	1146.645867	14.718605
19.957598	1152.297118	14.723623
20.091614	1152.852984	14.728640
20.605278	1172.276928	14.733658
20.402014	1180.019545	14.738675
20.362890	1182.058766	14.743693
20.398213	1183.867949	14.748711
20.488832	1178.747697	14.753728
20.324741	1184.536641	14.758746
20.336035	1172.049418	14.763763
20.397450	1176.736874	14.768781
20.060399	1187.562980	14.773799
20.768491	1182.179461	14.778816
20.271091	1181.804085	14.783834
20.307254	1175.643274	14.788851
20.710217	1172.419280	14.793869
20.342337	1185.629949	14.798887
20.537323	1188.517388	14.803904
20.761706	1215.746557	14.808922
20.788725	1211.960020	14.813939
20.747877	1208.639434	14.818957
20.651617	1220.396924	14.823975
20.610751	1213.275256	14.828992
20.321441	1218.414886	14.834010
20.234373	1213.374044	14.839027
20.617357	1207.575071	14.844045
20.727796	1214.199252	14.849063
20.867573	1211.131033	14.854080
20.547999	1227.045084	14.859098
21.052983	1227.733615	14.864115
21.251198	1233.064955	14.869133
21.022653	1232.235226	14.874151
21.336092	1212.545362	14.879168
21.321744	1217.863077	14.884186
21.083160	1213.427230	14.889203
21.148884	1209.035481	14.894221
21.001500	1206.411653	14.899239
21.353162	1203.748495	14.904256
21.117802	1199.848718	14.909274
21.236719	1210.210370	14.914291
21.523871	1207.708283	14.919309
21.268433	1212.865136	14.924327
21.226659	1206.162903	14.929344
21.413888	1206.137533	14.934362
21.304252	1206.589657	14.939379
21.365694	1203.902510	14.944397
20.990599	1208.910283	14.949415
21.354304	1207.132508	14.954432
21.037396	1201.147077	14.959450
21.075636	1210.017011	14.964467
21.542572	1205.215529	14.969485
21.072810	1207.285905	14.974503
21.382904	1203.506431	14.979520
21.398898	1203.988931	14.984538
21.184558	1207.145723	14.989555
21.244609	1202.101389	14.994573
21.601378	1218.487674	14.999591
21.571999	1205.442213	15.004608
21.117690	1212.160303	15.009626
21.602355	1226.099103	15.014643
21.899027	1234.047145	15.019661
22.090136	1233.246743	15.024679
21.766089	1218.943010	15.029696
21.516053	1202.520004	15.034714
21.630851	1207.004541	15.039731
22.079563	1209.728320	15.044749
21.650157	1209.326331	15.049767
21.515512	1200.156866	15.054784
21.952075	1206.936091	15.059802
21.633025	1207.703592	15.064819
21.840504	1201.869905	15.069837
21.540117	1197.321072	15.074855
21.699066	1198.370042	15.079872
21.572598	1206.785765	15.084890
21.805151	1220.362380	15.089907
21.999368	1221.868099	15.094925
21.874743	1238.013653	15.099943
22.226506	1227.865225	15.104960
21.994194	1223.173619	15.109978
22.068241	1216.694716	15.114995
22.347828	1197.913207	15.120013
21.933863	1203.452991	15.125031
21.905974	1197.717333	15.130048
21.894075	1198.367440	15.135066
21.835780	1199.477185	15.140083
21.895153	1218.421704	15.145101
22.099849	1233.706838	15.150119
22.147413	1231.956607	15.155136
21.941735	1233.787987	15.160154
21.967411	1232.036263	15.165171
22.389909	1228.240139	15.170189
22.244558	1231.144966	15.175207
21.944767	1226.647599	15.180224
21.962600	1222.748804	15.185242
22.032158	1221.477597	15.190259
22.134837	1228.060944	15.195277
21.877085	1234.808699	15.200295
22.016039	1226.929314	15.205312
22.200993	1237.048953	15.210330
22.207537	1253.762160	15.215347
22.623535	1247.059695	15.220365
22.483452	1245.489350	15.225383
22.757457	1221.135644	15.230400
22.811010	1223.385896	15.235418
22.646459	1216.795325	15.240435
22.809219	1218.129090	15.245453
22.573608	1224.493657	15.250471
22.924685	1215.066986	15.255488
22.714668	1212.947216	15.260506
22.384567	1217.063311	15.265523
22.482399	1216.960622	15.270541
22.840938	1223.332312	15.275559
22.344424	1219.373416	15.280576
22.737449	1218.458085	15.285594
22.446766	1224.714451	15.290611
22.553072	1219.425450	15.295629
22.724964	1218.723111	15.300647
22.528403	1223.321807	15.305664
22.597302	1215.395761	15.310682
22.667836	1216.790467	15.315699
22.732129	1228.598935	15.320717
22.667368	1238.231198	15.325735
22.869219	1241.244672	15.330752
22.920180	1248.699957	15.335770
22.983633	1256.678755	15.340787
23.049717	1241.218693	15.345805
22.850699	1253.046766	15.350823
23.056504	1254.216324	15.355840
23.206083	1247.461128	15.360858
23.065527	1241.824423	15.365875
23.030415	1240.652829	15.370893
23.115913	1257.644691	15.375911
22.655641	1248.836591	15.380928
23.025755	1246.601462	15.385946
22.757536	1254.537151	15.390963
22.818979	1241.964010	15.395981
22.548640	1248.009935	15.400999
22.642889	1243.768961	15.406016
23.013762	1251.225997	15.411034
22.868703	1268.037943	15.416051
23.232198	1273.917900	15.421069
23.357468	1282.308907	15.426087
23.548696	1281.649031	15.431104
23.671103	1269.824418	15.436122
23.723549	1271.838645	15.441139
23.594586	1251.506649	15.446157
23.369787	1256.156486	15.451175
23.289098	1241.766766	15.456192
23.529034	1241.929122	15.461210
23.320675	1240.803143	15.466227
23.547471	1247.161227	15.471245
23.276620	1246.964866	15.476263
23.364851	1259.177652	15.481280
23.890675	1264.656325	15.486298
23.752044	1272.046561	15.491315
23.520407	1258.674712	15.496333
23.660098	1255.420675	15.501351
23.526653	1262.926187	15.506368
23.945882	1260.579776	15.511386
23.804699	1251.426717	15.516403
23.841605	1243.185490	15.521421
23.629480	1249.678852	15.526439
23.539496	1243.951885	15.531456
24.014340	1238.658937	15.536474
23.474864	1250.995735	15.541491
24.124939	1255.727864	15.546509
24.072540	1236.741445	15.551527
23.577818	1241.860373	15.556544
23.815881	1230.509934	15.561562
23.741723	1250.551379	15.566579
23.800693	1262.452485	15.571597
24.111781	1260.045637	15.576615
24.262258	1263.091638	15.581632
24.399192	1238.184630	15.586650
23.980486	1249.944751	15.591667
23.886942	1234.621755	15.596685
24.143203	1235.243206	15.601703
23.970186	1231.909856	15.606720
24.037632	1229.694534	15.611738
24.180514	1242.972246	15.616755
24.283200	1246.358433	15.621773
24.298456	1234.565763	15.626791
24.060621	1232.497445	15.631808
24.109011	1235.236337	15.636826
24.139466	1254.307733	15.641843
24.272127	1262.663254	15.646861
24.130407	1258.149939	15.651879
24.130089	1270.591959	15.656896
24.582211	1260.822945	15.661914
24.393147	1265.539701	15.666931
24.044200	1265.996808	15.671949
24.298134	1275.564117	15.676967
24.171338	1266.297646	15.681984
24.462209	1264.864989	15.687002
24.170537	1278.037920	15.692019
24.587845	1268.399861	15.697037
24.221566	1276.301012	15.702055
23.933759	1274.370095	15.707072
24.396053	1266.728087	15.712090
24.374930	1287.731643	15.717107
24.563050	1295.289826	15.722125
24.531330	1300.141952	15.727143
24.525316	1304.311490	15.732160
25.025336	1298.189173	15.737178
24.790722	1304.950843	15.742195
24.977951	1297.916561	15.747213
25.014283	1297.559099	15.752231
24.617117	1303.467782	15.757248
24.763078	1294.541160	15.762266
24.627177	1307.361164	15.767283
24.589381	1297.820100	15.772301
24.771240	1302.109705	15.777319
24.729782	1299.391945	15.782336
24.818580	1289.061828	15.787354
25.098717	1303.894785	15.792371
24.622446	1295.721184	15.797389
25.158525	1302.251300	15.802407
24.581008	1305.253293	15.807424
24.967212	1286.298515	15.812442
24.909354	1303.327157	15.817459
25.139365	1294.932276	15.822477
25.050192	1301.687578	15.827495
24.748980	1303.801315	15.832512
24.659247	1309.490986	15.837530
24.607388	1326.997785	15.842547
25.019460	1326.570231	15.847565
24.970938	1329.134640	15.852583
25.040190	1324.821800	15.857600
25.442985	1327.290610	15.862618
25.468918	1328.019889	15.867635
25.606670	1319.096581	15.872653
25.489369	1326.694724	15.877671
25.478332	1331.777682	15.882688
25.645763	1324.126599	15.887706
25.564130	1327.748045	15.892723
25.474684	1328.538948	15.897741
25.566125	1320.263060	15.902759
25.372664	1322.711313	15.907776
25.575856	1315.088564	15.912794
25.449304	1325.222835	15.917811
25.846456	1322.848969	15.922829
25.449159	1325.763644	15.927847
25.149737	1326.758999	15.932864
25.491313	1317.066128	15.937882
25.703558	1321.876288	15.942899
25.655295	1325.005603	15.947917
25.657446	1316.166167	15.952935
25.444271	1322.334542	15.957952
25.640630	1319.962430	15.962970
25.491476	1327.350104	15.967987
25.558343	1337.172832	15.973005
26.150356	1335.176927	15.978023
26.083219	1350.318216	15.983040
26.298782	1329.693245	15.988058
25.936445	1323.007428	15.993075
26.071995	1313.593946	15.998093
26.013063	1302.910337	16.003111
25.904397	1310.818454	16.008128
25.968723	1307.271380	16.013146
26.146133	1308.418086	16.018163
26.051663	1307.572057	16.023181
26.281865	1303.992793	16.028199
26.041772	1312.994699	16.033216
26.345547	1309.554035	16.038234
26.046235	1305.916391	16.043251
26.227042	1304.147632	16.048269
26.097847	1300.427884	16.053287
25.807277	1312.882173	16.058304
26.367013	1328.220420	16.063322
26.442652	1340.060558	16.068339
26.516979	1343.365243	16.073357
26.512633	1334.803639	16.078375
26.095789	1327.788269	16.083392
26.382898	1329.510502	16.088410
26.587555	1340.078906	16.093427
26.266646	1335.997201	16.098445
26.481897	1329.876358	16.103463
26.227999	1333.326334	16.108480
27.115661	1335.899894	16.113498
26.772695	1337.491818	16.118515
26.394411	1323.713495	16.123533
26.362978	1334.188314	16.128551
26.580811	1332.767745	16.133568
26.843545	1332.196419	16.138586
26.776774	1333.071755	16.143603
26.813587	1340.279037	16.148621
26.803837	1324.915306	16.153639
26.704209	1335.711648	16.158656
26.981331	1333.432458	16.163674
26.782315	1329.306162	16.168691
26.506682	1331.245198	16.173709
26.714569	1336.921029	16.178727
26.507200	1338.434990	16.183744
26.935943	1333.484285	16.188762
26.758338	1333.909478	16.193779
26.633398	1338.410917	16.198797
26.953852	1331.386842	16.203815
26.525531	1334.425945	16.208832
26.807879	1326.140882	16.213850
26.912081	1331.058698	16.218867
26.427427	1340.044817	16.223885
26.846434	1341.553482	16.228903
27.131088	1362.621465	16.233920
27.217919	1359.419466	16.238938
27.069045	1359.363926	16.243955
26.924194	1369.158348	16.248973
27.104196	1362.233106	16.253991
26.985684	1366.243733	16.259008
26.927722	1365.569999	16.264026
27.400654	1354.577816	16.269043
26.855210	1363.185832	16.274061
27.022026	1369.543662	16.279079
27.486351	1389.450059	16.284096
27.408005	1380.437698	16.289114
27.921536	1393.718731	16.294131
27.658651	1376.340988	16.299149
27.912963	1360.468936	16.304167
27.654343	1366.923983	16.309184
27.377152	1354.001714	16.314202
27.375564	1352.742278	16.319219
27.595651	1347.588721	16.324237
27.776900	1348.023389	16.329255
27.478909	1348.438203	16.334272
27.695870	1345.150487	16.339290
27.782795	1348.821585	16.344307
27.515795	1352.347749	16.349325
27.760476	1358.404103	16.354343
27.558438	1372.886660	16.359360
27.740216	1386.551750	16.364378
27.757676	1376.840860	16.369395
27.913469	1380.129307	16.374413
28.264425	1379.511875	16.379431
28.073590	1385.948619	16.384448
27.900006	1383.469254	16.389466
28.115919	1384.321799	16.394483
28.060649	1385.947191	16.399501
28.177916	1369.158861	16.404519
28.043250	1372.129661	16.409536
27.761316	1375.322088	16.414554
28.203420	1380.109165	16.419571
27.823509	1376.763980	16.424589
28.104396	1378.667561	16.429607
27.918389	1383.530300	16.434624
27.923393	1381.530805	16.439642
28.059114	1378.876210	16.444659
27.858198	1382.409942	16.449677
28.298152	1378.017594	16.454695
27.953600	1382.326673	16.459712
28.076001	1395.708694	16.464730
28.377628	1399.036776	16.469747
28.468369	1405.537137	16.474765
28.473608	1398.078620	16.479783
28.486191	1397.670365	16.484800
28.637599	1400.267427	16.489818
28.890861	1393.005635	16.494835
28.430113	1401.797283	16.499853
28.729137	1388.023676	16.504871
28.464987	1400.305159	16.509888
28.708404	1399.667739	16.514906
28.687893	1395.506355	16.519923
28.621244	1405.763435	16.524941
28.835854	1393.283311	16.529959
28.746167	1396.349422	16.534976
28.895056	1394.154448	16.539994
28.533819	1388.981785	16.545011
28.678970	1390.855088	16.550029
28.923827	1395.691367	16.555047
28.662938	1391.869390	16.560064
28.835585	1389.074035	16.565082
28.876493	1388.163853	16.570099
29.133546	1393.017009	16.575117
29.205775	1388.022172	16.580135
29.051787	1387.740711	16.585152
28.981898	1382.814290	16.590170
29.185778	1382.128693	16.595187
29.202032	1398.801079	16.600205
29.265697	1387.009332	16.605223
29.221288	1390.037630	16.610240
29.118024	1387.523786	16.615258
29.386415	1391.145161	16.620275
29.076772	1399.642499	16.625293
29.172130	1392.450948	16.630311
29.471354	1395.596359	16.635328
29.058675	1393.421146	16.640346
29.008999	1388.483896	16.645363
28.802314	1394.699256	16.650381
29.148511	1397.468784	16.655399
28.881786	1383.673115	16.660416
28.909378	1397.836180	16.665434
29.416502	1413.178499	16.670451
29.268158	1428.900626	16.675469
29.511336	1419.059814	16.680487
29.614114	1426.137318	16.685504
29.505063	1418.680000	16.690522
29.602872	1427.547674	16.695539
29.224204	1429.329769	16.700557
29.372408	1415.735834	16.705575
29.599901	1419.773825	16.710592
29.418303	1419.547722	16.715610
29.542504	1416.490308	16.720627
29.203360	1435.244785	16.725645
29.671699	1436.961430	16.730663
29.691290	1445.707423	16.735680
29.516240	1454.056521	16.740698
29.590237	1441.600036	16.745715
29.560079	1447.910595	16.750733
29.634646	1446.708225	16.755751
29.913185	1452.173977	16.760768
30.230736	1463.908405	16.765786
30.939977	1460.355688	16.770803
30.408156	1454.045118	16.775821
30.413042	1439.149318	16.780839
30.762964	1443.615856	16.785856
30.292268	1435.581019	16.790874
30.831868	1437.760268	16.795891
30.474813	1439.958072	16.800909
30.364281	1421.987734	16.805927
30.328401	1414.961997	16.810944
30.044042	1420.546930	16.815962
30.492925	1415.072004	16.820979
30.447503	1436.536079	16.825997
30.819242	1428.993631	16.831015
30.543321	1417.010064	16.836032
30.333633	1415.015406	16.841050
30.394996	1403.841735	16.846067
30.388811	1418.156867	16.851085
30.416477	1434.121898	16.856103
30.541582	1438.943375	16.861120
30.229242	1436.856264	16.866138
30.596087	1437.365714	16.871155
30.242634	1443.673899	16.876173
30.503187	1432.703443	16.881191
30.846382	1433.968375	16.886208
30.380502	1435.539323	16.891226
30.883681	1431.352631	16.896243
30.552479	1431.690269	16.901261
30.818716	1431.243555	16.906279
30.757860	1433.358454	16.911296
30.714368	1439.142876	16.916314
30.699392	1439.351775	16.921331
30.916342	1465.744830	16.926349
31.034461	1464.250998	16.931367
31.181073	1461.362698	16.936384
30.882499	1471.263347	16.941402
31.331703	1467.535578	16.946419
31.544430	1462.379265	16.951437
31.179934	1443.321438	16.956455
31.171203	1441.082874	16.961472
30.932618	1431.845444	16.966490
31.595526	1454.807196	16.971507
31.289463	1436.826698	16.976525
31.600473	1428.817147	16.981543
31.122362	1421.809123	16.986560
31.151393	1430.604331	16.991578
31.324690	1425.871877	16.996595
31.466636	1450.782462	17.001613
31.532997	1463.610048	17.006631
31.456788	1456.139006	17.011648
31.597493	1459.968940	17.016666
31.789223	1448.995695	17.021683
31.268488	1443.105731	17.026701
31.252931	1449.934733	17.031719
31.765717	1456.708535	17.036736
31.652788	1467.881577	17.041754
31.694689	1453.349315	17.046771
31.727210	1457.493222	17.051789
31.700569	1452.095843	17.056807
31.876052	1456.171195	17.061824
31.601308	1461.854550	17.066842
31.975449	1458.010868	17.071859
31.857642	1462.861157	17.076877
31.785134	1444.998668	17.081895
31.888058	1458.554833	17.086912
31.849179	1453.841363	17.091930
31.834839	1460.103244	17.096947
31.989655	1457.542324	17.101965
32.043245	1452.725747	17.106983
32.062811	1450.348245	17.112000
31.840441	1461.825229	17.117018
31.826728	1449.276176	17.122035
32.246601	1456.189771	17.127053
32.007578	1465.154186	17.132071
32.075289	1476.891412	17.137088
31.876277	1476.896536	17.142106
32.162075	1479.343012	17.147123
32.218829	1475.791642	17.152141
32.328472	1475.660224	17.157159
32.336501	1476.412160	17.162176
32.165634	1476.186640	17.167194
32.219178	1474.949167	17.172211
32.566520	1472.485891	17.177229
32.176626	1480.105230	17.182247
32.671121	1476.965230	17.187264
32.517388	1480.119915	17.192282
32.497011	1474.160472	17.197299
32.450134	1478.375405	17.202317
32.321369	1499.189987	17.207335
32.804731	1500.480927	17.212352
33.117516	1510.835088	17.217370
33.077254	1500.562029	17.222387
33.254432	1497.924564	17.227405
32.472553	1483.002307	17.232423
32.944605	1474.322764	17.237440
32.700697	1483.351778	17.242458
33.085813	1498.919895	17.247475
33.068304	1495.950498	17.252493
32.792020	1489.294060	17.257511
33.134685	1489.455550	17.262528
32.935497	1509.816063	17.267546
33.262939	1500.194316	17.272563
33.222282	1510.930623	17.277581
33.364241	1509.035597	17.282599
33.056954	1483.975770	17.287616
32.982528	1488.472431	17.292634
32.843148	1496.666827	17.297651
32.795178	1498.391809	17.302669
33.022840	1503.776635	17.307687
33.398017	1504.746909	17.312704
33.154474	1509.074730	17.317722
33.499079	1507.572918	17.322739
33.206063	1511.916412	17.327757
32.829763	1510.736727	17.332775
33.347933	1504.895575	17.337792
33.593928	1531.296137	17.342810
33.962126	1530.087266	17.347827
33.738737	1525.563774	17.352845
33.382828	1515.173681	17.357863
33.709690	1522.377114	17.362880
33.701003	1533.148693	17.367898
33.682663	1532.395557	17.372915
33.809794	1521.713271	17.377933
33.893804	1540.330877	17.382951
34.215131	1517.014930	17.387968
33.632521	1518.119785	17.392986
33.903195	1521.799080	17.398003
33.845122	1523.205267	17.403021
34.005784	1525.502394	17.408039
34.439661	1517.583869	17.413056
33.995866	1517.251181	17.418074
34.117796	1524.018080	17.423091
34.453628	1528.794455	17.428109
34.153451	1511.775882	17.433127
34.166229	1495.764948	17.438144
33.896632	1494.919561	17.443162
34.061044	1515.134048	17.448179
34.111548	1516.269107	17.453197
34.054882	1516.818766	17.458215
34.005428	1517.283373	17.463232
34.176681	1528.409797	17.468250
33.976217	1523.912430	17.473267
34.347684	1520.939642	17.478285
34.034371	1526.375471	17.483303
34.077930	1535.481717	17.488320
34.263134	1550.026301	17.493338
34.300104	1553.809656	17.498355
34.843283	1544.525386	17.503373
34.397109	1558.000514	17.508391
34.874435	1545.164170	17.513408
34.661573	1546.057016	17.518426
34.896498	1551.602859	17.523443
34.812369	1549.751565	17.528461
34.654392	1553.592004	17.533479
34.728418	1549.704687	17.538496
34.909343	1555.107112	17.543514
34.602243	1552.401010	17.548531
34.642226	1549.068541	17.553549
34.630343	1546.503713	17.558567
35.034011	1553.743262	17.563584
34.848722	1557.824837	17.568602
35.350145	1551.854159	17.573619
35.407630	1555.488842	17.578637
35.233383	1552.406806	17.583655
35.153276	1541.271816	17.588672
35.129127	1541.028300	17.593690
35.098245	1538.228825	17.598707
35.413357	1535.175997	17.603725
35.367694	1541.378138	17.608743
35.409345	1533.284790	17.613760
35.157015	1533.381812	17.618778
35.220195	1539.230498	17.623795
35.461258	1544.406427	17.628813
35.378445	1562.567040	17.633831
35.338977	1565.122114	17.638848
35.728716	1564.127783	17.643866
35.423808	1569.899635	17.648883
35.655883	1563.499932	17.653901
35.684406	1569.876020	17.658919
35.858314	1563.906812	17.663936
35.576831	1566.396056	17.668954
35.658064	1565.940602	17.673971
35.674266	1563.557734	17.678989
35.624930	1569.582936	17.684007
35.846455	1560.034597	17.689024
35.870601	1577.507440	17.694042
35.826968	1569.788430	17.699059
36.183289	1560.111078	17.704077
36.034232	1563.510279	17.709095
35.977530	1559.648938	17.714112
36.134708	1556.384069	17.719130
35.945035	1557.858900	17.724147
36.077455	1555.431986	17.729165
35.988746	1559.881033	17.734183
36.272882	1558.158128	17.739200
36.143324	1557.526949	17.744218
36.335959	1564.962077	17.749235
36.372362	1551.745196	17.754253
36.314107	1567.776167	17.759271
36.252301	1557.296795	17.764288
35.871724	1557.483557	17.769306
36.014192	1571.086815	17.774323
36.235132	1572.629482	17.779341
36.275136	1588.398930	17.784359
36.331602	1587.199153	17.789376
36.374667	1583.024042	17.794394
36.521647	1589.152571	17.799411
36.886212	1584.526980	17.804429
36.496006	1590.372019	17.809447
36.696728	1578.538534	17.814464
36.623828	1585.186146	17.819482
36.593334	1589.132649	17.824499
36.706598	1579.055375	17.829517
36.703033	1604.709593	17.834535
36.837452	1613.605564	17.839552
37.011177	1613.016290	17.844570
37.181692	1607.725187	17.849587
37.437653	1608.511666	17.854605
37.024723	1607.962840	17.859623
37.577421	1604.679713	17.864640
37.358095	1585.702397	17.869658
37.160380	1581.817943	17.874675
37.732022	1567.692343	17.879693
37.354927	1572.487177	17.884711
37.193585	1575.044323	17.889728
37.288755	1563.359823	17.894746
37.056730	1575.104236	17.899763
37.288746	1565.608093	17.904781
37.122781	1571.343159	17.909799
36.991212	1581.730396	17.914816
37.012282	1585.685683	17.919834
37.223221	1604.296915	17.924851
37.803025	1601.086467	17.929869
37.575201	1600.404628	17.934887
37.594343	1597.075994	17.939904
37.983375	1603.859330	17.944922
37.667014	1608.160653	17.949939
37.564873	1602.345014	17.954957
37.476956	1605.911660	17.959975
37.754881	1599.252775	17.964992
37.983592	1600.824474	17.970010
38.056156	1596.603530	17.975027
38.222825	1592.674878	17.980045
37.873449	1597.885601	17.985063
37.889346	1597.879153	17.990080
38.091544	1599.756816	17.995098
37.901012	1601.573525	18.000115
37.799620	1598.129416	18.005133
37.770414	1602.357992	18.010151
37.786649	1591.952288	18.015168
37.876817	1608.895338	18.020186
37.831273	1630.224662	18.025203
37.919137	1627.057870	18.030221
37.967893	1636.265676	18.035239
37.651411	1627.676462	18.040256
38.034038	1631.406143	18.045274
38.301527	1660.971875	18.050291
38.694961	1656.302507	18.055309
38.609694	1661.275817	18.060327
38.614606	1658.139684	18.065344
38.521346	1661.509195	18.070362
38.640509	1659.716746	18.075379
39.061997	1651.134456	18.080397
39.325560	1650.611801	18.085415
39.254968	1640.364930	18.090432
39.330828	1631.469014	18.095450
38.903820	1624.498104	18.100467
39.115891	1620.030825	18.105485
39.146985	1614.539971	18.110503
38.937095	1617.299257	18.115520
39.258082	1614.924181	18.120538
38.701497	1612.608591	18.125555
38.746269	1603.934374	18.130573
39.021103	1611.209457	18.135591
39.193478	1615.541666	18.140608
39.210226	1614.563425	18.145626
38.978509	1613.081443	18.150643
38.907508	1611.109464	18.155661
38.982794	1616.158143	18.160679
38.817862	1622.559199	18.165696
39.251487	1637.683992	18.170714
39.222456	1640.370027	18.175731
39.387662	1649.186118	18.180749
39.511977	1649.794003	18.185767
39.341149	1645.672009	18.190784
39.701448	1646.243182	18.195802
39.519363	1647.695504	18.200819
39.473225	1651.106423	18.205837
39.831396	1651.075191	18.210855
39.530535	1648.153471	18.215872
39.613377	1643.667425	18.220890
39.423524	1646.046626	18.225907
39.297799	1650.766002	18.230925
39.700112	1654.334555	18.235943
39.675317	1676.117200	18.240960
40.002018	1679.438043	18.245978
39.583645	1679.154683	18.250995
40.044117	1675.612797	18.256013
40.166657	1672.212694	18.261031
39.850747	1686.669123	18.266048
40.155737	1673.771445	18.271066
40.041812	1682.616452	18.276083
40.053666	1679.487038	18.281101
40.378242	1681.245235	18.286119
39.740129	1677.433679	18.291136
40.047175	1672.262467	18.296154
40.110293	1682.674227	18.301171
40.061292	1677.347401	18.306189
40.343244	1695.208399	18.311207
40.435511	1701.639735	18.316224
40.983757	1696.827003	18.321242
40.790676	1706.007966	18.326259
40.681350	1680.456770	18.331277
40.769403	1678.601754	18.336295
40.594632	1668.652431	18.341312
40.783224	1666.274860	18.346330
40.539032	1669.657161	18.351347
41.008244	1678.070172	18.356365
40.860667	1675.712438	18.361383
40.504688	1676.249459	18.366400
40.971705	1683.842755	18.371418
41.009405	1687.796495	18.376435
40.872929	1690.945215	18.381453
40.973673	1697.607823	18.386471
41.008947	1701.729292	18.391488
40.654742	1698.302219	18.396506
41.107956	1692.046162	18.401523
41.421556	1694.172321	18.406541
40.947752	1698.137532	18.411559
41.302794	1702.852119	18.416576
41.468905	1687.336467	18.421594
41.271190	1693.012662	18.426611
41.138461	1689.526083	18.431629
41.041646	1699.556855	18.436647
41.287664	1694.047707	18.441664
41.376899	1683.385759	18.446682
41.347148	1704.703908	18.451699
41.414377	1722.919392	18.456717
41.496030	1723.107570	18.461735
41.450438	1734.940132	18.466752
41.508275	1726.243998	18.471770
41.495725	1718.310710	18.476787
41.596500	1725.884356	18.481805
41.727103	1721.431718	18.486823
41.566509	1726.996660	18.491840
41.915115	1710.209420	18.496858
41.691149	1732.058981	18.501875
42.001948	1740.342744	18.506893
42.142468	1739.364473	18.511911
42.086302	1750.312963	18.516928
42.439797	1742.385981	18.521946
42.205179	1736.361124	18.526963
42.439411	1737.232311	18.531981
42.512145	1718.403717	18.536999
42.343072	1718.953098	18.542016
42.883778	1714.410510	18.547034
42.347322	1709.963998	18.552051
42.191363	1706.910005	18.557069
42.256896	1703.138624	18.562087
42.042112	1710.757033	18.567104
42.769388	1725.558089	18.572122
42.674240	1728.914936	18.577139
42.769610	1729.370136	18.582157
42.956080	1715.540073	18.587175
42.396872	1714.948141	18.592192
42.702244	1705.943312	18.597210
42.885884	1727.337183	18.602227
42.927512	1727.254821	18.607245
42.721187	1713.444131	18.612263
43.050707	1726.854349	18.617280
43.384235	1716.012949	18.622298
43.131388	1715.281312	18.627315
42.787350	1700.269806	18.632333
42.942184	1707.582128	18.637351
42.850182	1705.215974	18.642368
43.367049	1724.675913	18.647386
42.948759	1720.746057	18.652403
43.196236	1730.253300	18.657421
43.256425	1716.718558	18.662439
43.133889	1724.257919	18.667456
43.477251	1718.450753	18.672474
43.204046	1722.570157	18.677491
43.218456	1723.223803	18.682509
43.332477	1731.777155	18.687527
43.327502	1731.822195	18.692544
43.336246	1729.577940	18.697562
43.478678	1735.430112	18.702579
43.145903	1736.360934	18.707597
43.532826	1739.820638	18.712615
43.452460	1751.875901	18.717632
43.377441	1765.875977	18.722650
43.564020	1759.058132	18.727667
43.440040	1763.042994	18.732685
43.741866	1756.542291	18.737703
43.482998	1766.208203	18.742720
43.687929	1765.869270	18.747738
44.159262	1774.750886	18.752755
44.180324	1783.823208	18.757773
44.229668	1781.617497	18.762791
44.138404	1785.307574	18.767808
44.255111	1777.196159	18.772826
44.593071	1780.692327	18.777843
44.428930	1781.899562	18.782861
44.709267	1780.693016	18.787879
44.286076	1765.366204	18.792896
44.589456	1760.658961	18.797914
44.307171	1762.269225	18.802931
44.458504	1767.713633	18.807949
44.482735	1770.389297	18.812967
44.017980	1779.926709	18.817984
44.472282	1779.851213	18.823002
44.319994	1774.419801	18.828019
44.417207	1771.447103	18.833037
44.593574	1768.940044	18.838055
44.142347	1774.884627	18.843072
44.657592	1788.037370	18.848090
44.740578	1797.849454	18.853107
44.922046	1806.910189	18.858125
45.102741	1804.544536	18.863143
44.631695	1805.272663	18.868160
45.026427	1807.909426	18.873178
44.945522	1808.979257	18.878195
44.902477	1812.326313	18.883213
45.385601	1803.187664	18.888231
45.067722	1811.045636	18.893248
45.182483	1808.753105	18.898266
45.358838	1809.296080	18.903283
45.211853	1829.477892	18.908301
45.777337	1824.084308	18.913319
45.637545	1824.436322	18.918336
45.828351	1829.237986	18.923354
45.860594	1803.349757	18.928371
45.785866	1799.844100	18.933389
45.989465	1796.425036	18.938407
45.544359	1800.902062	18.943424
45.813598	1793.549643	18.948442
45.733231	1796.356018	18.953459
45.378460	1802.221646	18.958477
45.962674	1790.297729	18.963495
45.971601	1802.287852	18.968512
46.001791	1792.108052	18.973530
45.956336	1794.800771	18.978547
46.118103	1795.122143	18.983565
46.104856	1799.247342	18.988583
46.142669	1803.670390	18.993600
46.240034	1816.574237	18.998618
46.331695	1808.778768	19.003635
46.188115	1824.597358	19.008653
46.492167	1807.236280	19.013671
46.403618	1819.249643	19.018688
46.270897	1813.990964	19.023706
46.411909	1812.111808	19.028723
46.169243	1819.388425	19.033741
46.565643	1809.138134	19.038759
46.230285	1818.598237	19.043776
46.248583	1813.838575	19.048794
46.322960	1814.050794	19.053811
46.316273	1816.848122	19.058829
46.266892	1820.066699	19.063847
46.387291	1840.171180	19.068864
46.375457	1841.038235	19.073882
46.797762	1842.567666	19.078899
46.464280	1845.835653	19.083917
46.908117	1849.028081	19.088935
46.756156	1847.723817	19.093952
47.183622	1862.005349	19.098970
47.140898	1869.172110	19.103987
47.263480	1874.646120	19.109005
47.425848	1873.581150	19.114023
47.521025	1880.073103	19.119040
47.402316	1879.894452	19.124058
47.819530	1870.324545	19.129075
47.350138	1844.933488	19.134093
47.588472	1840.875977	19.139111
47.751830	1841.660085	19.144128
47.647079	1836.758189	19.149146
47.660670	1829.720923	19.154163
47.263331	1836.131021	19.159181
47.673670	1844.790490	19.164199
47.917021	1867.258148	19.169216
47.886195	1861.818405	19.174234
48.185613	1861.051614	19.179251
47.736899	1860.304369	19.184269
47.882409	1860.860327	19.189287
47.922684	1862.670739	19.194304
47.604540	1858.323076	19.199322
47.663990	1864.409121	19.204339
47.672659	1865.787357	19.209357
48.164099	1857.296917	19.214375
48.066141	1863.312567	19.219392
47.921798	1864.657083	19.224410
48.154472	1866.146262	19.229427
48.537585	1885.123031	19.234445
48.532109	1883.692933	19.239463
48.603048	1892.943677	19.244480
48.715280	1891.457079	19.249498
48.905510	1890.437102	19.254515
48.316435	1880.530259	19.259533
48.657555	1879.411281	19.264551
48.700388	1890.741122	19.269568
48.641470	1891.027383	19.274586
48.834132	1885.844726	19.279603
48.524120	1896.922361	19.284621
48.920756	1884.248315	19.289639
49.017670	1887.950959	19.294656
48.947644	1887.366603	19.299674
48.935083	1883.276214	19.304691
48.676346	1889.542122	19.309709
48.874360	1882.469963	19.314727
48.918733	1881.578865	19.319744
49.089077	1882.942143	19.324762
48.962952	1881.560369	19.329779
48.926099	1892.747105	19.334797
48.996721	1909.494503	19.339815
49.281986	1914.546701	19.344832
49.420722	1910.857639	19.349850
49.793567	1911.269262	19.354867
49.252599	1922.716660	19.359885
49.461760	1904.816057	19.364903
49.925253	1901.679927	19.369920
49.685640	1909.108840	19.374938
49.625633	1901.315602	19.379955
49.852486	1908.119628	19.384973
50.006927	1908.702457	19.389991
49.675444	1910.845695	19.395008
49.708775	1905.476417	19.400026
50.015613	1899.531922	19.405043
49.945106	1910.199824	19.410061
49.860394	1906.828476	19.415079
49.860431	1910.919614	19.420096
49.982167	1930.596817	19.425114
50.440594	1942.952786	19.430131
49.974707	1931.695169	19.435149
50.531154	1936.988304	19.440167
50.494773	1931.513235	19.445184
50.252325	1937.813474	19.450202
50.605657	1940.523652	19.455219
50.293604	1940.177011	19.460237
50.131776	1939.146427	19.465255
50.224918	1937.561015	19.470272
50.343341	1932.596544	19.475290
50.623491	1942.850099	19.480307
50.395777	1949.471138	19.485325
50.797922	1962.264797	19.490343
50.781321	1964.454331	19.495360
50.811136	1962.499079	19.500378
50.720306	1954.043187	19.505395
50.730530	1961.837458	19.510413
50.808290	1960.116005	19.515431
51.129391	1955.846724	19.520448
50.734824	1966.337214	19.525466
51.395021	1971.519479	19.530483
51.228492	1987.337704	19.535501
51.679527	1989.529339	19.540519
51.717955	1977.553523	19.545536
51.329187	1970.165483	19.550554
51.631933	1967.395335	19.555571
51.671901	1965.045873	19.560589
51.580240	1959.603964	19.565607
52.080907	1955.490387	19.570624
51.649989	1949.769609	19.575642
51.791597	1941.571700	19.580659
51.660414	1943.703431	19.585677
51.735359	1967.777105	19.590695
52.117342	1971.256185	19.595712
51.847990	1980.203082	19.600730
51.726333	1979.065053	19.605747
52.016548	1980.291561	19.610765
52.072998	1974.498342	19.615783
52.374672	1975.588303	19.620800
51.954148	1981.229053	19.625818
52.324380	1971.414101	19.630835
52.183920	1982.020404	19.635853
52.447924	1975.756981	19.640871
52.712789	1973.294293	19.645888
52.590027	1981.483043	19.650906
52.374873	1973.217022	19.655923
52.614832	1968.143044	19.660941
52.614732	1967.019142	19.665959
52.598924	1962.425715	19.670976
52.498781	1970.152829	19.675994
52.747043	1968.286999	19.681011
52.573834	1973.811203	19.686029
52.803193	1977.621469	19.691047
53.147671	1965.687113	19.696064
52.651986	1970.223744	19.701082
52.759857	1964.505481	19.706099
53.079671	1972.717404	19.711117
52.768623	1966.694875	19.716135
52.891801	1968.560864	19.721152
53.259221	1991.238478	19.726170
52.989146	1985.489086	19.731187
53.045309	1997.675086	19.736205
53.162573	1990.960353	19.741223
53.488377	1990.256906	19.746240
53.184563	1994.003880	19.751258
53.460879	1995.083474	19.756275
53.500966	1995.744297	19.761293
53.361925	1997.022985	19.766311
53.306101	1993.894872	19.771328
53.351844	2014.213126	19.776346
53.446685	2012.607346	19.781363
53.789710	2025.043514	19.786381
53.326089	2034.739558	19.791399
53.579817	2031.609395	19.796416
53.511783	2030.235706	19.801434
53.646347	2044.195423	19.806451
54.148509	2050.743684	19.811469
53.934041	2067.747126	19.816487
54.514634	2055.133824	19.821504
54.373019	2051.220670	19.826522
54.824917	2052.117647	19.831539
54.777225	2038.900496	19.836557
54.301104	2042.651996	19.841575
54.632544	2042.980714	19.846592
54.652449	2053.329797	19.851610
54.510878	2038.186011	19.856627
54.583047	2045.099570	19.861645
54.593544	2038.286350	19.866663
54.768527	2034.862130	19.871680
54.419720	2039.637065	19.876698
54.616743	2039.658109	19.881715
54.750458	2049.803301	19.886733
54.601283	2045.382724	19.891751
55.015998	2053.818746	19.896768
55.048924	2069.635525	19.901786
55.308629	2067.820940	19.906803
55.191936	2073.828355	19.911821
54.925606	2076.275010	19.916839
55.216830	2070.559815	19.921856
54.934675	2077.527333	19.926874
55.135934	2072.247518	19.931891
55.313455	2073.751363	19.936909
55.355441	2076.159565	19.941927
55.722402	2063.340284	19.946944
55.277584	2065.270019	19.951962
55.558949	2063.010496	19.956979
55.593899	2078.791121	19.961997
55.486727	2081.697265	19.967015
55.732118	2081.476041	19.972032
55.924892	2088.893287	19.977050
55.962525	2089.127343	19.982067
55.911400	2086.533489	19.987085
55.890279	2086.480414	19.992103
56.358014	2079.495793	19.997120
56.049579	2080.188738	20.002138
56.586753	2089.676189	20.007155
56.394720	2071.248105	20.012173
56.759868	2079.039180	20.017191
56.702915	2068.689371	20.022208
56.783930	2081.655991	20.027226
56.807851	2073.800737	20.032243
56.798169	2060.243406	20.037261
56.365126	2056.767492	20.042279
56.490809	2049.579672	20.047296
56.601851	2054.210358	20.052314
56.708557	2064.772642	20.057331
56.615863	2073.649395	20.062349
56.530223	2075.984633	20.067367
56.625229	2074.928835	20.072384
56.300084	2078.454158	20.077402
56.580458	2076.901118	20.082419
56.757811	2088.230090	20.087437
56.789104	2101.738440	20.092455
56.999807	2094.910549	20.097472
57.131886	2099.243662	20.102490
57.133117	2097.539196	20.107507
57.217851	2100.086785	20.112525
57.091408	2107.788794	20.117543
57.446293	2104.341465	20.122560
57.348541	2123.591461	20.127578
57.467913	2124.850994	20.132595
57.799071	2124.181695	20.137613
57.795146	2129.333031	20.142631
57.659716	2125.133785	20.147648
57.764020	2132.638539	20.152666
57.749678	2124.545886	20.157683
57.948712	2127.586775	20.162701
57.860894	2125.565938	20.167719
58.104355	2121.736254	20.172736
57.852346	2123.848250	20.177754
58.057974	2118.810224	20.182771
57.926000	2127.237591	20.187789
57.632359	2142.670314	20.192807
58.094931	2141.919805	20.197824
58.520168	2149.098189	20.202842
58.586559	2154.083160	20.207859
58.415225	2150.059543	20.212877
58.351255	2150.340345	20.217895
58.488158	2151.193026	20.222912
58.695829	2148.166140	20.227930
58.526138	2152.498838	20.232947
59.131683	2148.192250	20.237965
58.894934	2148.869784	20.242983
58.671475	2151.738894	20.248000
58.949132	2163.238720	20.253018
59.197623	2177.148196	20.258035
59.204510	2168.307884	20.263053
59.278900	2179.673657	20.268071
59.412482	2169.451687	20.273088
59.295198	2165.826217	20.278106
59.323281	2166.815426	20.283123
59.680532	2156.758011	20.288141
59.499385	2166.326652	20.293159
59.551682	2159.015101	20.298176
59.389603	2159.468847	20.303194
59.444006	2161.725001	20.308211
59.925920	2155.278570	20.313229
59.287790	2169.402564	20.318247
59.499720	2160.242862	20.323264
59.746193	2170.352927	20.328282
59.655275	2159.630715	20.333299
59.972284	2160.470110	20.338317
59.774862	2162.959307	20.343335
59.977571	2159.956863	20.348352
59.802059	2172.151045	20.353370
59.931341	2187.900806	20.358387
60.291049	2190.390675	20.363405
60.099766	2197.134137	20.368423
60.060989	2187.470242	20.373440
60.304428	2192.131017	20.378458
60.443075	2194.809857	20.383475
60.315524	2199.721834	20.388493
60.266913	2198.738629	20.393511
60.552546	2190.024991	20.398528
60.570975	2205.641546	20.403546
60.429439	2220.737731	20.408563
60.803534	2218.495117	20.413581
60.299380	2225.304570	20.418599
60.752657	2221.903524	20.423616
60.569702	2221.450063	20.428634
60.766101	2227.531291	20.433651
61.236585	2239.366583	20.438669
61.137678	2250.475658	20.443687
61.233273	2244.226627	20.448704
61.628040	2254.364163	20.453722
61.698235	2244.495567	20.458739
62.057712	2238.569789	20.463757
61.640506	2245.206973	20.468775
61.657754	2228.483491	20.473792
61.568670	2219.129099	20.478810
61.763199	2230.118309	20.483827
61.921255	2232.417156	20.488845
61.600068	2235.033554	20.493863
61.759013	2230.242996	20.498880
62.081237	2241.368558	20.503898
61.716150	2236.021039	20.508915
62.076098	2228.424254	20.513933
61.503017	2239.027559	20.518951
61.919855	2242.039888	20.523968
62.171027	2233.552413	20.528986
62.073788	2250.587434	20.534003
62.145543	2245.054583	20.539021
62.017939	2261.049719	20.544039
62.200679	2258.961230	20.549056
62.570468	2250.330872	20.554074
62.636258	2256.228611	20.559091
62.964604	2253.773873	20.564109
62.833872	2250.425819	20.569127
62.809317	2250.471741	20.574144
62.768997	2245.695273	20.579162
62.847533	2263.858730	20.584179
62.894559	2249.225659	20.589197
62.796358	2261.178360	20.594215
62.996130	2271.083616	20.599232
63.086730	2277.189075	20.604250
63.152253	2287.637065	20.609267
63.457293	2280.147382	20.614285
63.167355	2289.478195	20.619303
63.278267	2280.596185	20.624320
63.515890	2282.752725	20.629338
63.206132	2278.892551	20.634355
63.489850	2276.914905	20.639373
63.293341	2285.191225	20.644391
63.463986	2294.413888	20.649408
63.463102	2303.729527	20.654426
63.849446	2303.192429	20.659443
63.478375	2305.151321	20.664461
63.578597	2308.000724	20.669479
63.656530	2306.983567	20.674496
64.193359	2295.977390	20.679514
63.653506	2310.290365	20.684531
64.411955	2321.861495	20.689549
64.395589	2330.870645	20.694567
64.168405	2339.850924	20.699584
64.494254	2330.817936	20.704602
64.659464	2334.881443	20.709619
64.916022	2325.735123	20.714637
64.679469	2336.309544	20.719655
64.879158	2326.727342	20.724672
65.024790	2320.583387	20.729690
64.827409	2311.678386	20.734707
64.768134	2294.315112	20.739725
64.857957	2311.964924	20.744743
64.800971	2323.669105	20.749760
64.976074	2322.630345	20.754778
64.912388	2326.464809	20.759795
65.174667	2326.991609	20.764813
65.138317	2330.554606	20.769831
64.923747	2326.799531	20.774848
64.819152	2324.357016	20.779866
64.992561	2338.963746	20.784883
65.316128	2345.670452	20.789901
65.529833	2358.233818	20.794919
65.657050	2351.762569	20.799936
65.611756	2345.431308	20.804954
65.679105	2352.637549	20.809971
65.876576	2354.870436	20.814989
65.579830	2352.660137	20.820007
65.818153	2344.510179	20.825024
66.103496	2341.512522	20.830042
65.795762	2354.194903	20.835059
66.216049	2363.640064	20.840077
66.153737	2375.279020	20.845095
66.453736	2369.534704	20.850112
66.356049	2372.890927	20.855130
66.460648	2385.378282	20.860147
66.679706	2377.553559	20.865165
66.457054	2380.300524	20.870183
66.439001	2377.350734	20.875200
66.940543	2370.382042	20.880218
66.502000	2376.316481	20.885235
66.829552	2370.770367	20.890253
66.583924	2371.009201	20.895271
66.601235	2372.691972	20.900288
67.168507	2372.511942	20.905306
67.040403	2368.844907	20.910323
66.812830	2387.180459	20.915341
67.156811	2397.093415	20.920359
67.460395	2405.695677	20.925376
67.470399	2399.950150	20.930394
67.482076	2402.353973	20.935411
67.808511	2391.486114	20.940429
67.901655	2400.119674	20.945447
67.589586	2404.213404	20.950464
67.852254	2394.589236	20.955482
67.717992	2394.827741	20.960499
67.894457	2398.109835	20.965517
67.629952	2394.571290	20.970535
67.721949	2394.736503	20.975552
67.654066	2393.124949	20.980570
67.588377	2404.616054	20.985587
67.798180	2399.331959	20.990605
68.245974	2414.157121	20.995623
68.028182	2423.572924	21.000640
68.223071	2427.328770	21.005658
68.060389	2424.377326	21.010675
68.424324	2423.837636	21.015693
68.143393	2428.598300	21.020711
67.991607	2422.375591	21.025728
68.490525	2425.289322	21.030746
68.623797	2424.161021	21.035763
68.947761	2436.338852	21.040781
69.112496	2436.343195	21.045799
68.869375	2443.941848	21.050816
69.234794	2440.838784	21.055834
69.188047	2443.406625	21.060851
68.861848	2435.253630	21.065869
68.832322	2437.407573	21.070887
68.869936	2434.324927	21.075904
69.196422	2436.302987	21.080922
69.056035	2434.495943	21.085939
69.004501	2434.269546	21.090957
69.183891	2447.475708	21.095975
69.306554	2453.651128	21.100992
69.543440	2458.531191	21.106010
69.489049	2473.158442	21.111027
69.622129	2460.839793	21.116045
69.567061	2468.997116	21.121063
69.731862	2471.773648	21.126080
69.935388	2496.258765	21.131098
69.621838	2498.284931	21.136115
69.874152	2496.377422	21.141133
70.206249	2488.103195	21.146151
70.088302	2495.995732	21.151168
70.255818	2488.438952	21.156186
70.301575	2496.146106	21.161203
70.498736	2505.235363	21.166221
70.611461	2514.188203	21.171239
70.861977	2521.387817	21.176256
71.215566	2518.829641	21.181274
71.211470	2527.269517	21.186291
70.941627	2514.744295	21.191309
71.047754	2499.404312	21.196327
71.124660	2499.788179	21.201344
71.105146	2502.401917	21.206362
71.186336	2507.777881	21.211379
71.184920	2510.083882	21.216397
71.314140	2507.441985	21.221415
71.315950	2511.239664	21.226432
71.468077	2508.182140	21.231450
71.498835	2510.383595	21.236467
71.468226	2503.332475	21.241485
71.666105	2503.362041	21.246503
71.335151	2500.972334	21.251520
71.341486	2499.189022	21.256538
71.353639	2514.110823	21.261555
71.925878	2523.814009	21.266573
72.149012	2529.120412	21.271591
71.800261	2528.175071	21.276608
71.797411	2525.954668	21.281626
72.225380	2529.365629	21.286643
72.133722	2522.784478	21.291661
72.008742	2525.383397	21.296679
71.977538	2532.310747	21.301696
72.458089	2553.981418	21.306714
72.513504	2561.249971	21.311731
72.554568	2562.033500	21.316749
72.384048	2555.159469	21.321767
72.216732	2561.295933	21.326784
72.565197	2558.053124	21.331802
72.733030	2567.881964	21.336819
72.925938	2586.611148	21.341837
73.423805	2585.240566	21.346855
73.410167	2596.015670	21.351872
73.705853	2585.181511	21.356890
73.405393	2571.351782	21.361907
73.233279	2563.863012	21.366925
73.540613	2550.212604	21.371943
73.206964	2560.193768	21.376960
73.167841	2565.083736	21.381978
73.120517	2573.788291	21.386995
73.103606	2592.552617	21.392013
73.405884	2590.231287	21.397031
73.342076	2595.521440	21.402048
73.998323	2603.152369	21.407066
74.045500	2607.753242	21.412083
73.949397	2621.461888	21.417101
74.297402	2613.657827	21.422119
74.379739	2608.527453	21.427136
74.306870	2607.288379	21.432154
74.448713	2603.227750	21.437171
74.440459	2607.442106	21.442189
74.474815	2604.352485	21.447207
74.518250	2609.837891	21.452224
74.535481	2604.464739	21.457242
74.499193	2613.832492	21.462259
74.527727	2610.154425	21.467277
74.981490	2615.484093	21.472295
74.771801	2634.778847	21.477312
75.049233	2633.264433	21.482330
74.931065	2639.573510	21.487347
75.070421	2634.497864	21.492365
75.308560	2636.854383	21.497383
75.302294	2642.999254	21.502400
75.095609	2629.671303	21.507418
75.238186	2628.965884	21.512435
75.205293	2631.434212	21.517453
75.407746	2643.840213	21.522471
75.505844	2656.777317	21.527488
76.265637	2660.331410	21.532506
76.083288	2655.426749	21.537523
75.922251	2666.875956	21.542541
76.202747	2655.139085	21.547559
75.966568	2655.554322	21.552576
76.149779	2653.574372	21.557594
76.067866	2649.927970	21.562611
76.019825	2659.558344	21.567629
76.448831	2653.279143	21.572647
76.089029	2657.899775	21.577664
76.224328	2670.136196	21.582682
76.753648	2680.774997	21.587699
76.640810	2682.356508	21.592717
76.868037	2675.570514	21.597735
76.762138	2681.950023	21.602752
76.825313	2673.635180	21.607770
76.888750	2683.586110	21.612787
76.736854	2677.357411	21.617805
76.773929	2669.191390	21.622823
76.758279	2693.543804	21.627840
77.131885	2708.205535	21.632858
77.197461	2707.099053	21.637875
77.067395	2710.061075	21.642893
77.496112	2708.849187	21.647911
77.309838	2718.023317	21.652928
77.383928	2710.078722	21.657946
77.316107	2721.286535	21.662963
77.468288	2730.753476	21.667981
77.914763	2730.869056	21.672999
78.068663	2724.336932	21.678016
78.220294	2723.315026	21.683034
78.203806	2726.446448	21.688051
78.109403	2730.557376	21.693069
78.152576	2728.307276	21.698087
78.097264	2729.014638	21.703104
78.072155	2727.823162	21.708122
78.268887	2737.895767	21.713139
78.390416	2749.786868	21.718157
78.770285	2761.983260	21.723175
78.619651	2755.434218	21.728192
78.700680	2764.091640	21.733210
78.663224	2752.577432	21.738227
78.647708	2759.021935	21.743245
78.866028	2754.888363	21.748263
79.008525	2747.610031	21.753280
78.965041	2756.554620	21.758298
79.377679	2772.695492	21.763315
79.190242	2775.173288	21.768333
79.518760	2773.942944	21.773351
79.785199	2765.330992	21.778368
79.387336	2770.028435	21.783386
79.983964	2774.402151	21.788403
79.666908	2775.650922	21.793421
80.176178	2772.344828	21.798439
80.106024	2774.963846	21.803456
79.878004	2765.081695	21.808474
80.053153	2760.489488	21.813491
79.868897	2772.662356	21.818509
80.126787	2773.812780	21.823527
80.091874	2772.800890	21.828544
80.227964	2776.348037	21.833562
80.371264	2792.578016	21.838579
80.247537	2800.127149	21.843597
80.370418	2801.517663	21.848615
80.419308	2806.554957	21.853632
80.640317	2799.468341	21.858650
80.613051	2797.077520	21.863667
80.493559	2813.202202	21.868685
81.036721	2812.778113	21.873703
81.067793	2820.728823	21.878720
80.973935	2816.516599	21.883738
81.269393	2808.279769	21.888755
81.321578	2815.343449	21.893773
81.559754	2825.153717	21.898791
81.299379	2818.674397	21.903808
81.104688	2822.731476	21.908826
81.541349	2836.774574	21.913843
81.293516	2851.805498	21.918861
81.642096	2850.170613	21.923879
82.221616	2849.373151	21.928896
82.200665	2852.566760	21.933914
82.359377	2840.822746	21.938931
82.091818	2842.833860	21.943949
82.252996	2837.399782	21.948967
82.263206	2843.304979	21.953984
82.162323	2846.545287	21.959002
82.468209	2857.922049	21.964019
82.492321	2865.890472	21.969037
82.739455	2868.829442	21.974055
82.849701	2870.546096	21.979072
82.503997	2867.342171	21.984090
82.657404	2866.187668	21.989107
82.512081	2871.683553	21.994125
82.483064	2866.841238	21.999143
82.676602	2887.027097	22.004160
83.040660	2898.151717	22.009178
83.410101	2892.350040	22.014195
83.140865	2897.217578	22.019213
83.411789	2900.001815	22.024231
83.734550	2884.857494	22.029248
83.690594	2895.950055	22.034266
83.869679	2892.576549	22.039283
83.860771	2898.738102	22.044301
84.146308	2891.503741	22.049319
84.037348	2897.250722	22.054336
83.901914	2897.492578	22.059354
84.068772	2897.651308	22.064371
84.217134	2892.180355	22.069389
84.189511	2880.281322	22.074407
84.489205	2880.787773	22.079424
84.143855	2895.226174	22.084442
84.349745	2906.747886	22.089459
84.411505	2912.703239	22.094477
84.792874	2916.109404	22.099495
84.599008	2904.552865	22.104512
84.701125	2911.091348	22.109530
84.815146	2908.683810	22.114547
84.529018	2919.205016	22.119565
84.825240	2927.526087	22.124583
84.882935	2932.941524	22.129600
84.978722	2945.242976	22.134618
85.243206	2938.807423	22.139635
84.918477	2947.838850	22.144653
85.159887	2945.739376	22.149671
85.617008	2967.558612	22.154688
85.369212	2978.536543	22.159706
85.879191	2961.101897	22.164723
85.558671	2969.497545	22.169741
85.487991	2974.186943	22.174759
85.963390	2978.520942	22.179776
85.766700	2997.721070	22.184794
86.412624	2991.718052	22.189811
86.198612	2997.285989	22.194829
86.463436	2990.817285	22.199847
87.085726	2988.726008	22.204864
86.876435	2988.733221	22.209882
87.157675	2981.479450	22.214899
87.213317	2983.148066	22.219917
86.964826	2993.262661	22.224935
87.147610	2980.781028	22.229952
87.241121	2985.207396	22.234970
87.409076	2984.187102	22.239987
87.127490	2980.961906	22.245005
87.697403	2975.608150	22.250023
87.438125	2984.519696	22.255040
86.923333	2984.198719	22.260058
86.979683	2973.948456	22.265075
87.626962	2984.561244	22.270093
87.017452	2981.165520	22.275111
87.672455	2986.615161	22.280128
87.534439	3006.235937	22.285146
87.622444	3008.637058	22.290163
87.525676	3006.275824	22.295181
87.502163	3006.969665	22.300199
87.827970	3023.588996	22.305216
87.646721	3034.703206	22.310234
88.144802	3035.944602	22.315251
88.456617	3040.268693	22.320269
87.992193	3044.976057	22.325287
88.413728	3059.155731	22.330304
88.503365	3055.256400	22.335322
88.643519	3058.716710	22.340339
88.903446	3061.747309	22.345357
89.159739	3050.983925	22.350375
89.127205	3048.756944	22.355392
88.755604	3056.379528	22.360410
89.241421	3073.814229	22.365427
89.174864	3078.475020	22.370445
89.273041	3088.593308	22.375463
89.601326	3078.334175	22.380480
89.511684	3081.125385	22.385498
89.621974	3075.922113	22.390515
89.654720	3080.382587	22.395533
89.631097	3079.966502	22.400551
90.195857	3072.065296	22.405568
90.077516	3078.461989	22.410586
89.965827	3084.190984	22.415603
90.296221	3077.596810	22.420621
90.035856	3088.468227	22.425639
90.060526	3094.795180	22.430656
90.516678	3109.010905	22.435674
90.270608	3106.358598	22.440691
90.392394	3103.676096	22.445709
90.320253	3104.674871	22.450727
90.691463	3112.805262	22.455744
90.240777	3128.750438	22.460762
90.657146	3129.230099	22.465779
91.298646	3136.020348	22.470797
91.123577	3131.384435	22.475815
91.507550	3134.057075	22.480832
91.664115	3132.118490	22.485850
91.356597	3125.740950	22.490867
91.531796	3135.446477	22.495885
91.647271	3146.954200	22.500903
92.026936	3153.443681	22.505920
91.789181	3149.513879	22.510938
92.130210	3155.045490	22.515955
92.288444	3151.854139	22.520973
92.080269	3154.627976	22.525991
92.296800	3150.042191	22.531008
92.206746	3155.369166	22.536026
92.151937	3144.621791	22.541043
92.199734	3152.596675	22.546061
92.400576	3155.351220	22.551079
92.715443	3161.445094	22.556096
92.476442	3185.242678	22.561114
92.645878	3180.391426	22.566131
92.914199	3183.633279	22.571149
92.695639	3181.404793	22.576167
92.823436	3175.519781	22.581184
92.757004	3189.559480	22.586202
93.207594	3199.452544	22.591219
92.872989	3210.186323	22.596237
93.104043	3213.106760	22.601255
93.266789	3201.325978	22.606272
93.575767	3226.712200	22.611290
93.657403	3234.142491	22.616307
93.911265	3230.580924	22.621325
93.741054	3233.893033	22.626343
93.534310	3241.195466	22.631360
93.596068	3246.203604	22.636378
93.964985	3255.744834	22.641395
94.119059	3263.007617	22.646413
94.219733	3275.568784	22.651431
94.160213	3256.005820	22.656448
94.259173	3268.610971	22.661466
94.596993	3284.436775	22.666483
94.815686	3293.807605	22.671501
94.487412	3294.305040	22.676519
95.235159	3286.252945	22.681536
94.750581	3289.247786	22.686554
95.310090	3288.371327	22.691571
95.557112	3287.840339	22.696589
95.012933	3288.618825	22.701607
95.532011	3282.963901	22.706624
95.375295	3291.508996	22.711642
95.540833	3306.605785	22.716659
95.934385	3302.117826	22.721677
95.924549	3311.917491	22.726695
96.168432	3299.872781	22.731712
95.744895	3314.221351	22.736730
96.011925	3311.930165	22.741747
95.859776	3312.915820	22.746765
96.097474	3302.427025	22.751783
96.286136	3297.961966	22.756800
96.513701	3313.992690	22.761818
96.244698	3329.802071	22.766835
96.550711	3336.240430	22.771853
96.893350	3338.710085	22.776871
97.477476	3333.247152	22.781888
97.115567	3341.470697	22.786906
97.012908	3338.455591	22.791923
97.239942	3328.173686	22.796941
96.910248	3342.780790	22.801959
97.332402	3334.840066	22.806976
97.336661	3326.793321	22.811994
97.543150	3330.732527	22.817011
97.618872	3332.130897	22.822029
97.270809	3351.119486	22.827047
97.637955	3355.221489	22.832064
97.512382	3360.284305	22.837082
97.470336	3355.079388	22.842099
98.172979	3369.446687	22.847117
97.895275	3390.299870	22.852135
98.299015	3392.237311	22.857152
98.215250	3391.540985	22.862170
98.183243	3387.555006	22.867187
98.525495	3378.652182	22.872205
98.534270	3393.752568	22.877223
98.806547	3392.769314	22.882240
99.145744	3404.607156	22.887258
99.277610	3405.007147	22.892275
99.378239	3400.253450	22.897293
98.975443	3405.497235	22.902311
99.439418	3399.283613	22.907328
99.188434	3401.503492	22.912346
98.981196	3397.899321	22.917363
99.714071	3412.410097	22.922381
99.544208	3431.138937	22.927399
100.062229	3430.137436	22.932416
100.142020	3433.508206	22.937434
100.007219	3440.108188	22.942451
100.268536	3434.678193	22.947469
100.060004	3439.093669	22.952487
100.394521	3431.068970	22.957504
100.485591	3427.718980	22.962522
100.349798	3428.963381	22.967539
100.675766	3427.988953	22.972557
100.429947	3432.429894	22.977575
100.477592	3439.522170	22.982592
100.572041	3447.963159	22.987610
100.612763	3457.888025	22.992627
101.023343	3449.312864	22.997645
100.650291	3456.381878	23.002663
101.189864	3468.991807	23.007680
101.404222	3481.753635	23.012698
101.010745	3483.079686	23.017715
101.284554	3478.344936	23.022733
101.316108	3482.381656	23.027751
101.540582	3497.203486	23.032768
101.977810	3507.756519	23.037786
101.747363	3507.568784	23.042803
102.376178	3503.653308	23.047821
102.321835	3508.144074	23.052839
101.946455	3510.601914	23.057856
102.170449	3499.830970	23.062874
102.227892	3496.546777	23.067891
102.496573	3500.222548	23.072909
102.436041	3526.214991	23.077927
102.730306	3536.114071	23.082944
102.732191	3531.025066	23.087962
102.583792	3537.169016	23.092979
102.817064	3526.539055	23.097997
102.720714	3532.783848	23.103015
103.446528	3552.594215	23.108032
103.335720	3561.920143	23.113050
103.296644	3557.638011	23.118067
103.484658	3556.080829	23.123085
103.370327	3553.038082	23.128103
103.494804	3554.268538	23.133120
103.570045	3566.291563	23.138138
103.998131	3591.023932	23.143155
104.548343	3581.945992	23.148173
104.479723	3588.128334	23.153191
104.297269	3586.206056	23.158208
104.446813	3579.927479	23.163226
104.231129	3577.146815	23.168243
104.609789	3578.980938	23.173261
104.787578	3579.837563	23.178279
104.827479	3582.394000	23.183296
104.979730	3592.593830	23.188314
104.658032	3607.823558	23.193331
104.939150	3593.140625	23.198349
105.178813	3607.929727	23.203367
105.365995	3601.573641	23.208384
105.499910	3593.133985	23.213402
105.456060	3601.666073	23.218419
105.550676	3611.932159	23.223437
105.706980	3624.923823	23.228455
105.731855	3625.202146	23.233472
105.997483	3628.567784	23.238490
105.685327	3629.179111	23.243507
106.040796	3630.103182	23.248525
106.140979	3650.917376	23.253543
106.418165	3652.086331	23.258560
106.404185	3645.989940	23.263578
106.251125	3663.498007	23.268595
106.592293	3650.837629	23.273613
106.755696	3665.996939	23.278631
106.708479	3680.588694	23.283648
107.202268	3682.355730	23.288666
107.193467	3687.396168	23.293683
107.182234	3687.028022	23.298701
107.102131	3681.414281	23.303719
107.216959	3677.646864	23.308736
107.547473	3692.458410	23.313754
107.718376	3711.889534	23.318771
107.633557	3710.069595	23.323789
107.852640	3706.433748	23.328807
107.536534	3709.035368	23.333824
108.124446	3702.837332	23.338842
108.066433	3727.244046	23.343859
108.524676	3726.083112	23.348877
108.349871	3734.419602	23.353895
108.118442	3736.982400	23.358912
108.439606	3737.088818	23.363930
108.451452	3742.910214	23.368947
108.776741	3758.941752	23.373965
108.949956	3764.502154	23.378983
108.576201	3758.253841	23.384000
109.122592	3757.859519	23.389018
108.848243	3757.491622	23.394035
109.004358	3754.503285	23.399053
109.603025	3770.145431	23.404071
109.423150	3782.332925	23.409088
109.728325	3777.315689	23.414106
109.742184	3790.615760	23.419123
109.658538	3780.318847	23.424141
110.068451	3777.890931	23.429159
109.880715	3780.771744	23.434176
110.298532	3795.085402	23.439194
110.445733	3807.360514	23.444211
110.686624	3811.845011	23.449229
110.591876	3808.635957	23.454247
110.531031	3811.010265	23.459264
110.807380	3807.077078	23.464282
110.552184	3807.517934	23.469299
110.578269	3811.068174	23.474317
110.849057	3827.525401	23.479335
110.742930	3835.336722	23.484352
111.175309	3835.405827	23.489370
111.065780	3837.523202	23.494387
111.641726	3849.473781	23.499405
111.768451	3857.039050	23.504423
111.781796	3864.100184	23.509440
111.936875	3846.412251	23.514458
111.856572	3859.444859	23.519475
111.752859	3847.643134	23.524493
111.757118	3858.101138	23.529511
112.060767	3883.320388	23.534528
112.358994	3890.273334	23.539546
112.544752	3886.087371	23.544563
112.730887	3889.467015	23.549581
112.557412	3888.761893	23.554599
112.890398	3897.771200	23.559616
113.039697	3900.489524	23.564634
112.874646	3913.342479	23.569651
112.997416	3912.544995	23.574669
113.130877	3910.703855	23.579687
113.429964	3919.069084	23.584704
113.803188	3922.949728	23.589722
113.874821	3934.065625	23.594739
114.088566	3930.392022	23.599757
114.229396	3936.372082	23.604775
114.522801	3931.651278	23.609792
114.506571	3926.091057	23.614810
114.228271	3931.697136	23.619827
114.579567	3920.306708	23.624845
114.755486	3924.491713	23.629863
114.405696	3932.961232	23.634880
114.592246	3927.899012	23.639898
114.794542	3940.616355	23.644915
114.637540	3952.918322	23.649933
114.994833	3960.840014	23.654951
114.627113	3966.963348	23.659968
114.896878	3957.382726	23.664986
114.980049	3983.562009	23.670003
115.225172	3991.534576	23.675021
115.564573	3990.193270	23.680039
115.521714	3992.914287	23.685056
115.945692	3995.202840	23.690074
115.932499	4011.043791	23.695091
115.981186	4013.694528	23.700109
116.183940	4015.351105	23.705127
116.184839	4010.159729	23.710144
116.458926	4011.902148	23.715162
116.439038	4018.104941	23.720179
116.508166	4038.283355	23.725197
116.841480	4044.253637	23.730215
116.636422	4039.386948	23.735232
117.030930	4033.525578	23.740250
117.006953	4033.161896	23.745267
117.340817	4032.078236	23.750285
117.276475	4031.931506	23.755303
117.085016	4034.059716	23.760320
117.551011	4051.501946	23.765338
117.596272	4053.439760	23.770355
117.792476	4059.600492	23.775373
117.584112	4042.989994	23.780391
117.568651	4053.014711	23.785408
118.230897	4068.252475	23.790426
118.205499	4084.719241	23.795443
117.952680	4085.688927	23.800461
118.246729	4085.586813	23.805479
118.186602	4085.274792	23.810496
118.506479	4095.336156	23.815514
118.729344	4113.271537	23.820531
118.958371	4118.201465	23.825549
119.125833	4111.914591	23.830567
118.758669	4122.446473	23.835584
119.268393	4127.404745	23.840602
119.467781	4143.261035	23.845619
119.596295	4143.498977	23.850637
119.824590	4129.915806	23.855655
119.793745	4139.000453	23.860672
119.687866	4133.662909	23.865690
119.864587	4149.244173	23.870707
119.884983	4161.576784	23.875725
120.005044	4165.370250	23.880743
120.059142	4166.363941	23.885760
120.487222	4179.205540	23.890778
121.016051	4186.016879	23.895795
120.702561	4194.508879	23.900813
121.278076	4186.901453	23.905831
121.014351	4191.465669	23.910848
121.201376	4184.098184	23.915866
121.221633	4193.132663	23.920883
121.292342	4184.752769	23.925901
121.498719	4195.607133	23.930919
121.511588	4218.706598	23.935936
121.722488	4213.455973	23.940954
121.900040	4215.497122	23.945971
121.769065	4219.465256	23.950989
122.199190	4209.112925	23.956007
121.899599	4224.303755	23.961024
122.267682	4237.916880	23.966042
122.376434	4250.710603	23.971059
122.334759	4244.294495	23.976077
122.322853	4244.465908	23.981095
122.470091	4263.084174	23.986112
122.590710	4269.862330	23.991130
123.084166	4277.630909	23.996147
122.757739	4269.981402	24.001165
123.358563	4283.706453	24.006183
123.344509	4298.938284	24.011200
123.728923	4298.820420	24.016218
123.915481	4292.644506	24.021235
124.011490	4304.964711	24.026253
124.095949	4287.559674	24.031271
124.089376	4300.231562	24.036288
124.129213	4294.276823	24.041306
124.519700	4304.903896	24.046323
124.573852	4318.739963	24.051341
125.020087	4307.124053	24.056359
124.691910	4317.277104	24.061376
124.689721	4318.999934	24.066394
124.759927	4322.552042	24.071411
124.737748	4317.866835	24.076429
125.190856	4307.962682	24.081447
124.895751	4329.272037	24.086464
125.156741	4331.892403	24.091482
125.293974	4344.294806	24.096499
125.330559	4346.936578	24.101517
125.514541	4359.343065	24.106535
125.700303	4363.788810	24.111552
125.644741	4377.615530	24.116570
126.175761	4378.260147	24.121587
125.982698	4384.717781	24.126605
126.487658	4371.560334	24.131623
126.281729	4382.353145	24.136640
126.435468	4402.932266	24.141658
126.540048	4405.937660	24.146675
126.583361	4402.693813	24.151693
126.969020	4402.457612	24.156711
127.106161	4419.467999	24.161728
127.379115	4410.349650	24.166746
127.507197	4423.056834	24.171763
127.419969	4415.618878	24.176781
127.675352	4410.467929	24.181799
127.644232	4413.106746	24.186816
127.467515	4427.979737	24.191834
127.887935	4441.289046	24.196851
128.018098	4436.167483	24.201869
128.319106	4436.396560	24.206887
128.259459	4445.083718	24.211904
128.286627	4459.282709	24.216922
128.123746	4461.488148	24.221939
128.265722	4468.143148	24.226957
129.170666	4475.660988	24.231975
129.002871	4495.839838	24.236992
129.181077	4501.369750	24.242010
129.239363	4494.266787	24.247027
129.006886	4498.852694	24.252045
129.815792	4516.750577	24.257063
129.659806	4518.877702	24.262080
129.824299	4526.837904	24.267098
129.825352	4511.839788	24.272115
129.831256	4519.648256	24.277133
130.261960	4532.382606	24.282151
130.658798	4547.288333	24.287168
130.480893	4550.076695	24.292186
130.777694	4543.445340	24.297203
131.147474	4548.456058	24.302221
130.665844	4549.219513	24.307239
130.879491	4555.299586	24.312256
131.171466	4556.141299	24.317274
131.289823	4560.932969	24.322291
131.184285	4580.754310	24.327309
131.653647	4572.415315	24.332327
131.433680	4572.718835	24.337344
131.720792	4574.389070	24.342362
131.986813	4587.273588	24.347379
131.747230	4611.873972	24.352397
132.261106	4604.538021	24.357415
132.316480	4608.391132	24.362432
132.282745	4601.748323	24.367450
132.501597	4615.102965	24.372467
132.486944	4635.070776	24.377485
132.906399	4628.162337	24.382503
132.601614	4630.772469	24.387520
132.657818	4648.365118	24.392538
133.384513	4653.479802	24.397555
133.203050	4658.782647	24.402573
133.416575	4662.179582	24.407591
133.437838	4656.609745	24.412608
133.245271	4659.271395	24.417626
133.851892	4671.290772	24.422643
133.761575	4691.502723	24.427661
134.082320	4682.107748	24.432679
134.081734	4689.537774	24.437696
134.365670	4695.228237	24.442714
134.335192	4702.955401	24.447731
134.419376	4715.650401	24.452749
134.623533	4710.907127	24.457767
134.692377	4712.541059	24.462784
134.810644	4721.461958	24.467802
135.395919	4727.699512	24.472819
135.599540	4734.779939	24.477837
135.547221	4729.648328	24.482855
135.758069	4733.595438	24.487872
135.366552	4734.702320	24.492890
135.733090	4733.310784	24.497907
135.883327	4751.391229	24.502925
136.530688	4759.297594	24.507943
136.468195	4761.922763	24.512960
136.352638	4768.997769	24.517978
136.523803	4757.286097	24.522995
136.610701	4776.401674	24.528013
136.802444	4786.004286	24.533031
137.034812	4789.578481	24.538048
136.725286	4802.392288	24.543066
137.065142	4793.405978	24.548083
136.914160	4804.215183	24.553101
137.478416	4819.336021	24.558119
137.599170	4827.841522	24.563136
137.561580	4824.963023	24.568154
137.925078	4828.344616	24.573171
137.485515	4833.950935	24.578189
137.929492	4832.826941	24.583207
138.082181	4847.196880	24.588224
138.371833	4857.479532	24.593242
138.651076	4864.388409	24.598259
138.604035	4870.404656	24.603277
138.664311	4866.355376	24.608295
138.960519	4878.992565	24.613312
138.944774	4899.657888	24.618330
139.098685	4895.424559	24.623347
138.972563	4893.932646	24.628365
139.383349	4913.587016	24.633383
139.773912	4919.526106	24.638400
139.514643	4937.239826	24.643418
140.191561	4920.169953	24.648435
140.227820	4929.055718	24.653453
140.404415	4948.691412	24.658471
140.662213	4951.558923	24.663488
140.570882	4961.017128	24.668506
140.642129	4945.930583	24.673523
140.788323	4952.752842	24.678541
141.002907	4963.177154	24.683559
141.161643	4975.728497	24.688576
141.442846	4976.323145	24.693594
141.443932	4980.581484	24.698611
141.479111	4974.670575	24.703629
141.815997	4974.825991	24.708647
141.533109	4987.155119	24.713664
141.650024	4998.131960	24.718682
142.002473	5003.110254	24.723699
142.231882	5005.435112	24.728717
142.220210	5018.493545	24.733735
142.389049	5027.705523	24.738752
142.609028	5047.509787	24.743770
142.750078	5033.408671	24.748787
142.982550	5040.987719	24.753805
142.880704	5036.696673	24.758823
143.084406	5034.892605	24.763840
142.957323	5057.191094	24.768858
143.366344	5051.452173	24.773875
143.485874	5056.713194	24.778893
143.623369	5075.444296	24.783911
143.731986	5080.166855	24.788928
143.952749	5090.490206	24.793946
144.023915	5087.655084	24.798963
143.951363	5094.345867	24.803981
144.429983	5102.668620	24.808999
144.501757	5114.231098	24.814016
144.680259	5117.421285	24.819034
144.993988	5112.304554	24.824051
145.150653	5134.223029	24.829069
144.987793	5137.009790	24.834087
145.409791	5145.762508	24.839104
145.359650	5153.920804	24.844122
145.263075	5152.171949	24.849139
145.414747	5163.785028	24.854157
145.228819	5173.599257	24.859175
145.879863	5180.129324	24.864192
145.635266	5199.213662	24.869210
146.289935	5202.487275	24.874227
146.766570	5211.594846	24.879245
146.411395	5227.964614	24.884263
146.850982	5230.018434	24.889280
147.055011	5239.853202	24.894298
147.223520	5234.574604	24.899315
147.231223	5235.668192	24.904333
147.165132	5244.535639	24.909351
147.525562	5259.618190	24.914368
147.824775	5265.653657	24.919386
147.696470	5268.418181	24.924403
148.073072	5278.945043	24.929421
148.390454	5292.717122	24.934439
148.424579	5289.519506	24.939456
148.364922	5285.925510	24.944474
148.357554	5285.282606	24.949491
148.974724	5292.891022	24.954509
149.050320	5309.195857	24.959527
149.205042	5297.524312	24.964544
149.468498	5308.433791	24.969562
149.797239	5309.627026	24.974579
149.896686	5309.101902	24.979597
149.754362	5301.671074	24.984615
149.862706	5298.995153	24.989632
149.554986	5306.962259	24.994650
149.985158	5322.175877	24.999667
150.527701	5330.051845	25.004685
150.351725	5333.555155	25.009703
150.082310	5339.172072	25.014720
150.542070	5352.481157	25.019738
151.024025	5359.450416	25.024755
150.841126	5368.176602	25.029773
150.928726	5374.912660	25.034791
150.789984	5376.731458	25.039808
150.826069	5387.480950	25.044826
150.964286	5402.413769	25.049843
151.378143	5409.323441	25.054861
151.827857	5418.072510	25.059879
151.931022	5414.789405	25.064896
152.169937	5435.763749	25.069914
152.190281	5444.193271	25.074931
152.924533	5440.539473	25.079949
152.581714	5441.042130	25.084967
153.153318	5438.885697	25.089984
153.094170	5435.794855	25.095002
152.954066	5441.750330	25.100019
153.242341	5447.616771	25.105037
153.596877	5460.320381	25.110055
153.748337	5456.469292	25.115072
153.858637	5466.153536	25.120090
153.716632	5470.041111	25.125107
153.959632	5463.126871	25.130125
154.376819	5472.342099	25.135143
154.487410	5474.084976	25.140160
154.333479	5478.968473	25.145178
154.582287	5481.128734	25.150195
154.909231	5490.643236	25.155213
154.782723	5485.730798	25.160231
154.671563	5496.977300	25.165248
154.811148	5518.458871	25.170266
155.160786	5510.664536	25.175283
155.849361	5519.749014	25.180301
155.593379	5530.690300	25.185319
155.904632	5543.238111	25.190336
155.733964	5544.595168	25.195354
155.749268	5551.247971	25.200371
156.031897	5561.687405	25.205389
156.104121	5575.289243	25.210407
156.283507	5580.350719	25.215424
156.471961	5597.046719	25.220442
156.661105	5608.707481	25.225459
156.902077	5605.989860	25.230477
156.714083	5621.150165	25.235495
157.163431	5628.243084	25.240512
157.305040	5624.641680	25.245530
157.846468	5641.741614	25.250547
158.055715	5662.999196	25.255565
157.977147	5667.786788	25.260583
158.222074	5660.516933	25.265600
158.485805	5656.191186	25.270618
158.897668	5650.352342	25.275635
159.149822	5665.485502	25.280653
159.183425	5685.104832	25.285671
159.535377	5682.274313	25.290688
159.580462	5679.070866	25.295706
159.430474	5684.674433	25.300723
159.669059	5682.388803	25.305741
159.499253	5688.977010	25.310759
159.800035	5673.038172	25.315776
159.550430	5674.468954	25.320794
159.820196	5689.407045	25.325811
159.721196	5695.789781	25.330829
160.192691	5716.892179	25.335847
160.231428	5728.732301	25.340864
160.549707	5738.628015	25.345882
160.882433	5750.729800	25.350899
160.981075	5757.977715	25.355917
160.891505	5765.708881	25.360935
161.173091	5764.019431	25.365952
161.314204	5782.238040	25.370970
161.120010	5791.145903	25.375987
162.036350	5792.359251	25.381005
161.716509	5809.082919	25.386023
162.421178	5807.706987	25.391040
162.399108	5819.922697	25.396058
162.275460	5816.412421	25.401075
162.870457	5821.950196	25.406093
163.051923	5840.307900	25.411111
163.427601	5843.352176	25.416128
163.455498	5840.659553	25.421146
163.516137	5853.307385	25.426163
163.816909	5834.204540	25.431181
163.482623	5843.606619	25.436199
163.723715	5838.647390	25.441216
163.645672	5845.348063	25.446234
163.589997	5860.766294	25.451251
163.774557	5864.704653	25.456269
163.960636	5878.628153	25.461287
164.284600	5886.463404	25.466304
164.545314	5894.543839	25.471322
164.752675	5912.289300	25.476339
165.042448	5915.598275	25.481357
164.984862	5928.964357	25.486375
164.892014	5927.616483	25.491392
165.047775	5945.029484	25.496410
165.296269	5959.338894	25.501427
165.716224	5964.084999	25.506445
165.762795	5986.399368	25.511463
165.992628	5978.556116	25.516480
166.291146	5985.854533	25.521498
165.960410	6010.936093	25.526515
166.808485	5999.443815	25.531533
166.895996	6019.891878	25.536551
166.978175	6020.970040	25.541568
167.313604	6038.731459	25.546586
167.835303	6045.240775	25.551603
168.120898	6037.494592	25.556621
167.769183	6035.949340	25.561639
167.892398	6041.239223	25.566656
168.106396	6049.892986	25.571674
168.051833	6059.155943	25.576691
168.301162	6065.344901	25.581709
168.633640	6071.464175	25.586727
168.924087	6080.783444	25.591744
168.772382	6099.350194	25.596762
168.997540	6096.681579	25.601779
169.277700	6090.150003	25.606797
168.889707	6120.907401	25.611815
169.320911	6123.463662	25.616832
169.683550	6125.060130	25.621850
169.554447	6151.350620	25.626867
169.820886	6152.364418	25.631885
169.956189	6163.758833	25.636903
170.014977	6169.321706	25.641920
170.471320	6180.073049	25.646938
170.504576	6179.955822	25.651955
171.013606	6192.588765	25.656973
171.120005	6213.467936	25.661991
171.220907	6199.905656	25.667008
171.203522	6209.330311	25.672026
171.393295	6229.001649	25.677044
171.629759	6222.932505	25.682061
171.914734	6243.743558	25.687079
172.345096	6262.429947	25.692096
172.335346	6259.807284	25.697114
172.553226	6262.269714	25.702132
172.908589	6257.664776	25.707149
173.143007	6280.552577	25.712167
172.808367	6292.537636	25.717184
173.372412	6287.098692	25.722202
173.277779	6286.532418	25.727220
173.993260	6294.383394	25.732237
173.482868	6313.005050	25.737255
173.884099	6310.402554	25.742272
174.023966	6307.546390	25.747290
174.010261	6320.173035	25.752308
174.237804	6333.211855	25.757325
174.328342	6348.600840	25.762343
174.600708	6344.477476	25.767360
174.692932	6347.896437	25.772378
174.987336	6369.590614	25.777396
174.932480	6367.963889	25.782413
175.368077	6364.845305	25.787431
175.481580	6388.051007	25.792448
175.882750	6393.528922	25.797466
175.747809	6404.719356	25.802484
175.884669	6393.334301	25.807501
175.979013	6412.055230	25.812519
176.300061	6430.249523	25.817536
176.697921	6426.222721	25.822554
176.318626	6438.349182	25.827572
176.460651	6457.601019	25.832589
176.712648	6458.011530	25.837607
177.045072	6475.888147	25.842624
177.252931	6487.158938	25.847642
177.440326	6498.314190	25.852660
177.741863	6507.134084	25.857677
177.783638	6521.879926	25.862695
177.896295	6525.304207	25.867712
178.163704	6529.178608	25.872730
178.472862	6554.700930	25.877748
178.674852	6554.918085	25.882765
178.668544	6564.156019	25.887783
178.651366	6577.735712	25.892800
179.207147	6573.196750	25.897818
179.305144	6588.141286	25.902836
179.842441	6590.705267	25.907853
179.783835	6598.905879	25.912871
179.634498	6604.454526	25.917888
179.972116	6616.704245	25.922906
180.126422	6626.610336	25.927924
180.398479	6633.023387	25.932941
180.710352	6643.426404	25.937959
180.728762	6650.324903	25.942976
181.152064	6658.037760	25.947994
181.333166	6672.512566	25.953012
181.664394	6680.884191	25.958029
181.812619	6686.758529	25.963047
181.713633	6697.888868	25.968064
182.247402	6692.083027	25.973082
182.320457	6712.423318	25.978100
182.605395	6706.986331	25.983117
182.782660	6711.635002	25.988135
182.627208	6717.986536	25.993152
182.909612	6730.113158	25.998170
182.659372	6742.828132	26.003188
183.173616	6735.966893	26.008205
183.232377	6757.378461	26.013223
183.364374	6764.702445	26.018240
184.002969	6776.754382	26.023258
183.730469	6798.613888	26.028276
184.190659	6802.796712	26.033293
184.048693	6793.659833	26.038311
184.361947	6824.324553	26.043328
184.525936	6817.172330	26.048346
184.853665	6837.878630	26.053364
185.115699	6835.708681	26.058381
185.618736	6846.957643	26.063399
185.405452	6860.169122	26.068416
185.874364	6859.603264	26.073434
185.755991	6870.896041	26.078452
185.978609	6884.399278	26.083469
186.325507	6881.651305	26.088487
186.210613	6880.810317	26.093504
186.500666	6898.914186	26.098522
186.427762	6914.411908	26.103540
186.757269	6911.202086	26.108557
186.931961	6931.408469	26.113575
186.810720	6946.566075	26.118592
187.312130	6953.903819	26.123610
187.427709	6962.327049	26.128628
187.686940	6971.912732	26.133645
188.072703	6973.007654	26.138663
188.041197	6983.716646	26.143680
188.444550	6992.316736	26.148698
188.475337	7010.788174	26.153716
189.077929	7003.523087	26.158733
189.105125	7003.655762	26.163751
189.190319	7030.666031	26.168768
189.353650	7037.925091	26.173786
189.251506	7041.702476	26.178804
189.802235	7037.050797	26.183821
190.051191	7050.558480	26.188839
190.062560	7060.784670	26.193856
190.064427	7059.232764	26.198874
190.217201	7082.966237	26.203892
190.390548	7090.690755	26.208909
190.384314	7093.432234	26.213927
190.548567	7114.139177	26.218944
190.745969	7120.371805	26.223962
190.885255	7146.506083	26.228980
191.270956	7161.114452	26.233997
191.847956	7170.136446	26.239015
191.871268	7177.429777	26.244032
192.227032	7186.005557	26.249050
192.020839	7202.986774	26.254068
192.369730	7213.198933	26.259085
192.945131	7219.222514	26.264103
192.915168	7230.146453	26.269120
193.492505	7235.953108	26.274138
193.317936	7254.175258	26.279156
193.534051	7247.541962	26.284173
193.940956	7262.591169	26.289191
193.771484	7272.133003	26.294208
194.311363	7282.345884	26.299226
194.321680	7296.401340	26.304244
194.228827	7303.494983	26.309261
194.557462	7307.854897	26.314279
194.591631	7320.884795	26.319296
194.846497	7333.270074	26.324314
195.482746	7341.124456	26.329332
195.272384	7353.242548	26.334349
195.791658	7356.216877	26.339367
195.858358	7372.310270	26.344384
195.956532	7387.962088	26.349402
196.059275	7391.901772	26.354420
196.315103	7402.991982	26.359437
196.704179	7413.782086	26.364455
196.649770	7420.565368	26.369472
197.172142	7434.493641	26.374490
197.131020	7443.329824	26.379508
197.144205	7454.796584	26.384525
197.774301	7462.408648	26.389543
198.005349	7477.850299	26.394560
198.349762	7481.778355	26.399578
198.564468	7472.979824	26.404596
198.533418	7496.402486	26.409613
198.764869	7514.904305	26.414631
198.468862	7517.120385	26.419648
199.150769	7517.906382	26.424666
199.363846	7535.679497	26.429684
199.246637	7542.162874	26.434701
199.620809	7540.908478	26.439719
199.530366	7563.499021	26.444736
199.842632	7568.893603	26.449754
199.771137	7575.704986	26.454772
200.057977	7592.649108	26.459789
200.874406	7587.546833	26.464807
200.609098	7596.235892	26.469824
200.737253	7614.988875	26.474842
201.227813	7627.496844	26.479860
201.245824	7627.022939	26.484877
201.663276	7632.027546	26.489895
201.929690	7645.447774	26.494912
201.999819	7636.399755	26.499930
202.324462	7643.797806	26.504948
201.993641	7658.050266	26.509965
202.339591	7664.769737	26.514983
202.647311	7680.093339	26.520000
202.877938	7697.618753	26.525018
203.112474	7704.114859	26.530036
203.078574	7711.423420	26.535053
203.934818	7730.456163	26.540071
204.039044	7743.169967	26.545088
203.940171	7742.935966	26.550106
203.965903	7745.927483	26.555124
204.180140	7764.506487	26.560141
204.795127	7770.789974	26.565159
204.813536	7792.698783	26.570176
205.059148	7781.620059	26.575194
205.530502	7793.238863	26.580212
205.365957	7811.259911	26.585229
205.581864	7817.095895	26.590247
205.696672	7821.120337	26.595264
206.173852	7837.802411	26.600282
206.240597	7853.356699	26.605300
205.931170	7859.604203	26.610317
206.977170	7873.520224	26.615335
206.392770	7876.589138	26.620352
207.130376	7895.826833	26.625370
207.152691	7911.179788	26.630388
207.263201	7914.058050	26.635405
207.573365	7934.311025	26.640423
207.716679	7942.554521	26.645440
207.702649	7957.428303	26.650458
208.020197	7982.775871	26.655476
208.098283	7989.130209	26.660493
208.555897	7996.678923	26.665511
208.483941	8000.512191	26.670528
209.247925	8030.079797	26.675546
209.674169	8031.212209	26.680564
209.477682	8050.055682	26.685581
209.834272	8048.978247	26.690599
209.822158	8063.342153	26.695616
209.971049	8078.942141	26.700634
210.455878	8088.522663	26.705652
210.579283	8101.076820	26.710669
211.005904	8100.046868	26.715687
211.238390	8124.511523	26.720704
211.189399	8126.908932	26.725722
211.795451	8146.929654	26.730740
211.587394	8148.501864	26.735757
211.741219	8154.393149	26.740775
211.866090	8168.399688	26.745792
212.281387	8176.071290	26.750810
212.527002	8189.106282	26.755828
212.866149	8213.350182	26.760845
213.165608	8209.933967	26.765863
213.257195	8217.863199	26.770880
213.508136	8234.004947	26.775898
213.957556	8237.390393	26.780916
213.742604	8243.341184	26.785933
213.916784	8259.260133	26.790951
214.012706	8265.410757	26.795968
214.623598	8267.577636	26.800986
214.979907	8264.549017	26.806004
214.794297	8283.345275	26.811021
215.225252	8293.483103	26.816039
215.309248	8298.229606	26.821056
215.314523	8304.444091	26.826074
215.646001	8315.574406	26.831092
215.899645	8332.416104	26.836109
215.782931	8330.947511	26.841127
216.409741	8349.074484	26.846144
216.535324	8361.368532	26.851162
216.504428	8367.953751	26.856180
216.634463	8385.634429	26.861197
216.858458	8390.890296	26.866215
217.099254	8415.229559	26.871232
216.982704	8423.887349	26.876250
217.239923	8447.128193	26.881268
217.477332	8461.433819	26.886285
217.916260	8474.987676	26.891303
218.088611	8495.279933	26.896320
218.311511	8513.533825	26.901338
218.821364	8504.870991	26.906356
219.132847	8538.964428	26.911373
219.249881	8532.926787	26.916391
219.360299	8554.791474	26.921408
219.945103	8563.153630	26.926426
220.239153	8576.570856	26.931444
220.395241	8595.807985	26.936461
220.848035	8593.951260	26.941479
220.833303	8605.896118	26.946496
221.128181	8624.766848	26.951514
221.578013	8617.661822	26.956532
221.072509	8630.737226	26.961549
221.440478	8646.936431	26.966567
221.608878	8659.972774	26.971584
221.862438	8667.537471	26.976602
222.538957	8678.387987	26.981620
222.679256	8689.624261	26.986637
222.982604	8686.566518	26.991655
222.889674	8706.205007	26.996672
223.250075	8715.519764	27.001690
223.842099	8718.071106	27.006708
223.547904	8743.176902	27.011725
223.651245	8745.278197	27.016743
223.856180	8761.230367	27.021760
224.068798	8772.405887	27.026778
224.453722	8779.848845	27.031796
224.669742	8802.153290	27.036813
224.808610	8804.226654	27.041831
225.242793	8818.611889	27.046848
225.394820	8836.986595	27.051866
225.834076	8839.697954	27.056884
225.594296	8861.372100	27.061901
226.099561	8873.583207	27.066919
226.421708	8879.248381	27.071936
226.572505	8896.134483	27.076954
226.583676	8901.398966	27.081972
226.894938	8924.515756	27.086989
227.114129	8930.368149	27.092007
227.638804	8934.250186	27.097024
227.886533	8951.301487	27.102042
228.083899	8949.834412	27.107060
228.287887	8965.473412	27.112077
228.676676	8975.535941	27.117095
228.673194	8982.248433	27.122112
228.509406	8992.065280	27.127130
228.832512	9013.685839	27.132148
228.858863	9020.056242	27.137165
228.828779	9032.752342	27.142183
229.402496	9041.838186	27.147200
229.409208	9057.531203	27.152218
229.868892	9066.344462	27.157236
229.712519	9079.611371	27.162253
230.069330	9112.748472	27.167271
230.669589	9125.367871	27.172288
230.619113	9141.820400	27.177306
231.092093	9143.424918	27.182324
231.117701	9174.229220	27.187341
231.638321	9175.335069	27.192359
231.702246	9193.423048	27.197376
231.987206	9204.842135	27.202394
232.245129	9221.305141	27.207412
232.266477	9240.844224	27.212429
232.305183	9252.922519	27.217447
232.906304	9262.492378	27.222464
233.138621	9283.272011	27.227482
233.515504	9293.510812	27.232500
233.489832	9304.150279	27.237517
233.841166	9325.323851	27.242535
234.746797	9327.723333	27.247552
234.606142	9345.426247	27.252570
235.078600	9351.989994	27.257588
235.084762	9356.702429	27.262605
235.235177	9375.297811	27.267623
235.370024	9381.400668	27.272640
235.330972	9396.029411	27.277658
236.092466	9416.149682	27.282676
236.199560	9424.232928	27.287693
235.866917	9433.961403	27.292711
236.364652	9446.773707	27.297728
236.566723	9475.871380	27.302746
237.108330	9478.570635	27.307764
237.128886	9501.706446	27.312781
237.234094	9513.285495	27.317799
237.995804	9531.177990	27.322816
238.274944	9538.497801	27.327834
238.559096	9547.167069	27.332852
238.952097	9566.850642	27.337869
239.210032	9560.961818	27.342887
239.359295	9566.620405	27.347904
239.531951	9588.564434	27.352922
240.238363	9594.783888	27.357940
240.455063	9596.134665	27.362957
240.507566	9600.083213	27.367975
240.499911	9606.732844	27.372992
240.675741	9626.422504	27.378010
240.763577	9631.917966	27.383028
240.881565	9634.035861	27.388045
241.201413	9655.360826	27.393063
241.157935	9658.173509	27.398080
241.371322	9687.216910	27.403098
241.662050	9686.888448	27.408116
241.923067	9708.905460	27.413133
241.900171	9727.151006	27.418151
242.570131	9749.980359	27.423168
242.586339	9766.613137	27.428186
242.707637	9788.465101	27.433204
242.954661	9808.376390	27.438221
243.253070	9825.471440	27.443239
243.939364	9836.173812	27.448256
243.507481	9852.712263	27.453274
243.915515	9876.458837	27.458292
244.531876	9883.598510	27.463309
244.582737	9913.986448	27.468327
245.159296	9915.017704	27.473344
245.316659	9923.101547	27.478362
245.669460	9929.317431	27.483380
246.307646	9939.322741	27.488397
246.194351	9941.104750	27.493415
246.381451	9946.123803	27.498432
246.090271	9968.518557	27.503450
246.648990	9983.975355	27.508468
246.854447	9995.828863	27.513485
247.011419	10005.943021	27.518503
247.419161	10014.339194	27.523520
247.574501	10034.911953	27.528538
247.776776	10035.461579	27.533556
247.745333	10055.480721	27.538573
247.964158	10081.727954	27.543591
248.516381	10091.868127	27.548608
248.717819	10110.932548	27.553626
248.853774	10122.878012	27.558644
249.337723	10149.771605	27.563661
249.561676	10158.193550	27.568679
249.961151	10171.462309	27.573696
249.783596	10185.821623	27.578714
250.286380	10211.165694	27.583732
250.435368	10218.694076	27.588749
250.423741	10243.975239	27.593767
251.313367	10252.559632	27.598784
251.340887	10276.803094	27.603802
251.794730	10287.215722	27.608820
251.990493	10295.724341	27.613837
251.713892	10308.468556	27.618855
251.747590	10335.805698	27.623872
252.224768	10355.410914	27.628890
252.876943	10386.889840	27.633908
252.998179	10391.124219	27.638925
253.161815	10414.144691	27.643943
253.794172	10431.427761	27.648960
254.024757	10450.408188	27.653978
254.177214	10453.484016	27.658996
254.607855	10463.456257	27.664013
254.558797	10479.507330	27.669031
254.932023	10491.211316	27.674048
255.144917	10512.408584	27.679066
255.903684	10527.860368	27.684084
255.854263	10540.151178	27.689101
256.068005	10551.602710	27.694119
256.334889	10564.288677	27.699136
256.301357	10581.563959	27.704154
256.577909	10601.315347	27.709172
257.140533	10609.792555	27.714189
257.125692	10629.404706	27.719207
257.524119	10647.002479	27.724224
257.942604	10663.432507	27.729242
258.016933	10677.111615	27.734260
258.441410	10695.639523	27.739277
258.326001	10715.780530	27.744295
258.680536	10723.562691	27.749312
258.766125	10743.972997	27.754330
259.183419	10763.967584	27.759348
259.366639	10784.947946	27.764365
259.823392	10801.363902	27.769383
260.184893	10806.420536	27.774400
260.636611	10823.122553	27.779418
261.037689	10836.876918	27.784436
261.247165	10853.366949	27.789453
261.490561	10862.213854	27.794471
261.373031	10872.152607	27.799488
261.574733	10895.471579	27.804506
261.601172	10904.111758	27.809524
262.182054	10923.592564	27.814541
262.208104	10936.496747	27.819559
262.553258	10946.210838	27.824576
262.801123	10969.205553	27.829594
262.931755	10992.588429	27.834612
263.387540	10989.248181	27.839629
263.466530	11019.821846	27.844647
263.482301	11020.036809	27.849664
263.744974	11046.306718	27.854682
263.995750	11058.986286	27.859700
264.439624	11079.764736	27.864717
264.587604	11111.515264	27.869735
264.986546	11122.611943	27.874752
264.961158	11147.186922	27.879770
265.432300	11181.424203	27.884788
266.073405	11193.509813	27.889805
266.166782	11214.741968	27.894823
266.552042	11220.068983	27.899840
267.055487	11237.944686	27.904858
267.107392	11259.579281	27.909876
267.449991	11272.221756	27.914893
267.605768	11280.506666	27.919911
267.857392	11308.357744	27.924928
268.284097	11318.599049	27.929946
268.228234	11340.325652	27.934964
268.689867	11344.275450	27.939981
268.956397	11371.260648	27.944999
269.148130	11389.419755	27.950016
269.662993	11410.607611	27.955034
269.655792	11423.114287	27.960052
270.012250	11440.316476	27.965069
270.510552	11459.932936	27.970087
270.648474	11469.245155	27.975104
271.202461	11478.107169	27.980122
271.402589	11500.477078	27.985140
271.769697	11501.708576	27.990157
271.737041	11529.150114	27.995175
271.847857	11548.874944	28.000192
272.263356	11562.060258	28.005210
272.318069	11579.443333	28.010228
272.641989	11597.569762	28.015245
272.362272	11622.171802	28.020263
273.181187	11646.893001	28.025280
273.688950	11668.477897	28.030298
273.860494	11687.693315	28.035316
274.354963	11700.359838	28.040333
274.433289	11714.702575	28.045351
274.867723	11731.624280	28.050368
275.093674	11750.964711	28.055386
275.480784	11769.169118	28.060404
275.784563	11776.622968	28.065421
275.816121	11798.590995	28.070439
276.475075	11814.194486	28.075456
276.785792	11830.941373	28.080474
276.943499	11847.173098	28.085492
277.293731	11857.863907	28.090509
277.581356	11866.163536	28.095527
277.632024	11881.056232	28.100544
278.116049	11887.207034	28.105562
277.931351	11908.834385	28.110580
278.557619	11918.882306	28.115597
278.776148	11951.073488	28.120615
279.151121	11957.340069	28.125632
279.656055	11973.497112	28.130650
279.782525	11988.516033	28.135668
280.064581	11991.208263	28.140685
280.179266	12009.711744	28.145703
280.198746	12015.168908	28.150720
280.553447	12033.470375	28.155738
280.650421	12046.711962	28.160756
281.158477	12058.624843	28.165773
281.390834	12073.383636	28.170791
281.164445	12089.824160	28.175808
281.929167	12104.579957	28.180826
282.154507	12127.256999	28.185844
282.545686	12129.742089	28.190861
282.754229	12158.068210	28.195879
283.197838	12173.896797	28.200896
283.647090	12179.262391	28.205914
283.346106	12206.357101	28.210932
283.660856	12215.415133	28.215949
284.093284	12233.656686	28.220967
284.188193	12247.634703	28.225984
284.465579	12271.625475	28.231002
284.541603	12308.467678	28.236020
284.967522	12315.496564	28.241037
285.204276	12337.814290	28.246055
285.661496	12363.691684	28.251072
286.078441	12389.271644	28.256090
286.134958	12403.449981	28.261108
286.815504	12426.327871	28.266125
286.861824	12447.812114	28.271143
287.016934	12467.514971	28.276160
287.354644	12477.248552	28.281178
287.453548	12502.903397	28.286196
287.964910	12524.692129	28.291213
288.117116	12553.907608	28.296231
288.601095	12574.548967	28.301248
289.185728	12592.326057	28.306266
289.379569	12613.875927	28.311284
289.722108	12626.840955	28.316301
289.897993	12652.601486	28.321319
289.951171	12673.758682	28.326336
290.502212	12687.023336	28.331354
290.628133	12709.115653	28.336372
291.532490	12724.936278	28.341389
291.352383	12737.828739	28.346407
291.675696	12754.218341	28.351424
292.285310	12774.725693	28.356442
292.383972	12803.307513	28.361460
292.887830	12813.491297	28.366477
293.026157	12828.928224	28.371495
293.132939	12846.485266	28.376512
293.856614	12856.282838	28.381530
293.602371	12882.961197	28.386548
294.461478	12884.639302	28.391565
294.587258	12907.589211	28.396583
294.571048	12932.149610	28.401600
295.083924	12940.978264	28.406618
294.850857	12975.334323	28.411636
295.426677	12995.160444	28.416653
295.607076	13023.833132	28.421671
296.229614	13030.691104	28.426688
296.498651	13045.964768	28.431706
296.595665	13072.096754	28.436724
297.112745	13084.306750	28.441741
297.404995	13096.832912	28.446759
297.858148	13121.260747	28.451776
298.122236	13128.863627	28.456794
298.230589	13160.815410	28.461812
298.395611	13167.114063	28.466829
298.521514	13187.966762	28.471847
298.644471	13211.527459	28.476864
299.168959	13235.042214	28.481882
299.541014	13256.182055	28.486900
299.688471	13277.757816	28.491917
299.932616	13300.409742	28.496935
300.158920	13322.784131	28.501952
300.797498	13334.751995	28.506970
301.121439	13359.482097	28.511988
300.993236	13375.330859	28.517005
301.103176	13401.046752	28.522023
301.810370	13416.864443	28.527040
302.490432	13427.158134	28.532058
302.615056	13450.432072	28.537076
302.907720	13471.928897	28.542093
303.178474	13489.089135	28.547111
303.550435	13503.517228	28.552128
303.925778	13524.481940	28.557146
304.136084	13542.675051	28.562164
304.324454	13556.093431	28.567181
304.298597	13574.027807	28.572199
304.971304	13608.577260	28.577216
305.114554	13619.606082	28.582234
305.243346	13646.950392	28.587252
305.702924	13670.780687	28.592269
306.189098	13696.482051	28.597287
306.155259	13722.197032	28.602304
306.616429	13748.890769	28.607322
306.763982	13774.164472	28.612340
306.954102	13799.948098	28.617357
307.929580	13827.456735	28.622375
307.712637	13847.260665	28.627392
308.166970	13866.591026	28.632410
308.230848	13900.775372	28.637428
308.676218	13925.223036	28.642445
308.793653	13949.814851	28.647463
309.456900	13962.950081	28.652480
309.799641	13985.895538	28.657498
310.279500	14026.774017	28.662516
310.317903	14035.030903	28.667533
310.989941	14060.410511	28.672551
310.959019	14084.741822	28.677568
311.362928	14096.950825	28.682586
311.570230	14127.217520	28.687604
311.776115	14144.297774	28.692621
312.644872	14168.234433	28.697639
312.850938	14194.785150	28.702656
313.343935	14209.542141	28.707674
313.464576	14240.624021	28.712692
313.873945	14250.320013	28.717709
313.813844	14275.255336	28.722727
314.004330	14300.658285	28.727744
314.554039	14324.529778	28.732762
314.761227	14356.253192	28.737780
315.041012	14368.865926	28.742797
315.505373	14397.631140	28.747815
315.813341	14432.233251	28.752832
316.165590	14436.162521	28.757850
316.465394	14470.037919	28.762868
316.500192	14493.184785	28.767885
317.200084	14515.053726	28.772903
317.290534	14543.006362	28.777920
317.756678	14566.844758	28.782938
318.162210	14587.003611	28.787956
318.663153	14608.752728	28.792973
319.288602	14622.035019	28.797991
319.155623	14645.739435	28.803008
319.142313	14664.308088	28.808026
319.752066	14680.928032	28.813044
319.839811	14708.509440	28.818061
320.438416	14726.053290	28.823079
320.696435	14749.297538	28.828096
321.211768	14760.596523	28.833114
321.220133	14794.722571	28.838132
321.707217	14808.574824	28.843149
322.025273	14814.973296	28.848167
322.221780	14841.331205	28.853184
322.339340	14859.041505	28.858202
322.376081	14888.669566	28.863220
322.714720	14913.880299	28.868237
323.274968	14929.495248	28.873255
323.592051	14963.568972	28.878272
323.664011	14987.916114	28.883290
324.192663	15000.455045	28.888308
324.404705	15034.587281	28.893325
324.730588	15053.893024	28.898343
324.846376	15086.750451	28.903360
325.356790	15100.731485	28.908378
326.066516	15141.623558	28.913396
326.374859	15157.798968	28.918413
326.725863	15171.316269	28.923431
326.922300	15209.770071	28.928448
327.292682	15218.368216	28.933466
327.495271	15243.668172	28.938484
327.442012	15269.094049	28.943501
328.119507	15293.183803	28.948519
327.982909	15323.638868	28.953536
328.847261	15355.179785	28.958554
329.147294	15389.225690	28.963572
329.396670	15426.864243	28.968589
329.996791	15435.935155	28.973607
329.966917	15470.494495	28.978624
330.669475	15496.241679	28.983642
331.087824	15517.955235	28.988660
331.268782	15541.374127	28.993677
332.022982	15561.566311	28.998695
331.987722	15583.681302	29.003712
332.685851	15611.199447	29.008730
332.841229	15620.823231	29.013748
333.442565	15654.747311	29.018765
333.787424	15666.735561	29.023783
333.827122	15688.215692	29.028800
334.250079	15708.871116	29.033818
334.511443	15725.962747	29.038836
334.988843	15753.270202	29.043853
335.026558	15770.406777	29.048871
335.251461	15803.606947	29.053888
335.487190	15818.009193	29.058906
335.983395	15845.581642	29.063924
336.000966	15874.390293	29.068941
336.570046	15902.412604	29.073959
336.868706	15931.852601	29.078976
337.167113	15970.303910	29.083994
337.556826	15994.057728	29.089012
337.920687	16017.524258	29.094029
338.351065	16041.009760	29.099047
338.521615	16072.383168	29.104064
339.128155	16099.255275	29.109082
339.377301	16124.009807	29.114100
339.738335	16157.676788	29.119117
340.203487	16177.525090	29.124135
340.123575	16207.706018	29.129152
340.796600	16230.979820	29.134170
341.161402	16252.074288	29.139188
341.319095	16279.129739	29.144205
341.798679	16298.685769	29.149223
342.030915	16326.381526	29.154240
342.169594	16353.173859	29.159258
342.911332	16382.899134	29.164276
342.883492	16404.950944	29.169293
343.393418	16423.751803	29.174311
343.554997	16457.863812	29.179328
344.027241	16488.231284	29.184346
344.397628	16508.221770	29.189364
344.366312	16529.949611	29.194381
344.948663	16556.282655	29.199399
345.130066	16580.169522	29.204416
345.475627	16607.586908	29.209434
345.862804	16627.544810	29.214452
346.215900	16673.742413	29.219469
346.577837	16685.775868	29.224487
346.885184	16713.426739	29.229504
347.323271	16750.190609	29.234522
347.675388	16778.225098	29.239540
347.787637	16801.456959	29.244557
348.524587	16824.897565	29.249575
348.898806	16863.382539	29.254592
349.194869	16882.573985	29.259610
349.921860	16901.463990	29.264628
349.992581	16928.826514	29.269645
350.385209	16948.052495	29.274663
350.855973	16977.177404	29.279680
350.790661	17006.159373	29.284698
351.618174	17028.201276	29.289716
351.522451	17056.289865	29.294733
351.997782	17080.258064	29.299751
352.243053	17111.873286	29.304768
352.436864	17141.257126	29.309786
353.097203	17158.588437	29.314804
353.492283	17199.353261	29.319821
353.370488	17222.848287	29.324839
353.973998	17265.579144	29.329856
354.551941	17296.406661	29.334874
354.701185	17319.830167	29.339892
354.847549	17358.960895	29.344909
355.662192	17376.728766	29.349927
356.092356	17403.647952	29.354944
356.437571	17438.176114	29.359962
357.091868	17453.502036	29.364980
357.142417	17481.400040	29.369997
357.829712	17507.605308	29.375015
358.127057	17539.739231	29.380032
358.222338	17564.565520	29.385050
358.914724	17575.715763	29.390068
359.022013	17607.433584	29.395085
359.438757	17624.823042	29.400103
359.541533	17656.508599	29.405120
359.511953	17693.017771	29.410138
360.293155	17716.114973	29.415156
360.103740	17758.819121	29.420173
361.056270	17779.083667	29.425191
361.327670	17818.423357	29.430208
361.430995	17848.480778	29.435226
362.213728	17867.034773	29.440244
362.388896	17904.714887	29.445261
362.956559	17926.559808	29.450279
363.668115	17946.240188	29.455296
363.578617	17975.593572	29.460314
364.150898	18008.821061	29.465332
364.499627	18034.857772	29.470349
364.885177	18060.227913	29.475367
365.149920	18072.756118	29.480384
365.499657	18111.008420	29.485402
365.905064	18129.462788	29.490420
366.306069	18167.370957	29.495437
366.399510	18185.568042	29.500455
366.793195	18212.838237	29.505472
367.123470	18251.505530	29.510490
367.713955	18276.983962	29.515508
367.795518	18299.917168	29.520525
368.234667	18325.734432	29.525543
368.573667	18351.986068	29.530560
368.622636	18372.377240	29.535578
369.328455	18393.758506	29.540596
369.456661	18431.345114	29.545613
369.942490	18451.950994	29.550631
370.132422	18485.649441	29.555648
370.584556	18507.301425	29.560666
370.993968	18540.159665	29.565684
370.993643	18576.760515	29.570701
371.405035	18605.500838	29.575719
371.894678	18649.737552	29.580736
372.054353	18679.432438	29.585754
372.538433	18711.329621	29.590772
372.859363	18751.391646	29.595789
373.136714	18780.628975	29.600807
374.058798	18809.909415	29.605824
374.224657	18855.165068	29.610842
374.863735	18879.599051	29.615860
375.004042	18916.593563	29.620877
375.660995	18942.230698	29.625895
376.302313	18965.675973	29.630912
376.266080	19003.795562	29.635930
377.003574	19022.293702	29.640948
377.110136	19050.820390	29.645965
377.808343	19071.328827	29.650983
378.688063	19092.453617	29.656000
378.790517	19121.774091	29.661018
379.517157	19135.803164	29.666036
379.528817	19163.674155	29.671053
379.746830	19185.045735	29.676071
380.076650	19205.268472	29.681088
380.677861	19237.098403	29.686106
381.318895	19251.895320	29.691124
381.270486	19280.020808	29.696141
381.582893	19303.941929	29.701159
382.093119	19333.658786	29.706176
382.317740	19373.944768	29.711194
382.696445	19395.209618	29.716212
382.978745	19419.531597	29.721229
383.088698	19455.551715	29.726247
383.794653	19481.775927	29.731264
383.923961	19519.629656	29.736282
384.213599	19544.661627	29.741300
384.485594	19588.276270	29.746317
384.802971	19620.016744	29.751335
385.533832	19655.176203	29.756352
385.667550	19697.216956	29.761370
386.287926	19725.446918	29.766388
386.453336	19764.373598	29.771405
386.351700	19793.566635	29.776423
387.129997	19839.958048	29.781440
387.601222	19880.855561	29.786458
388.314738	19910.834619	29.791476
389.206750	19945.061479	29.796493
389.198878	19974.724903	29.801511
389.786740	19997.748489	29.806528
389.989466	20037.509952	29.811546
390.070042	20063.876415	29.816564
390.488082	20092.846801	29.821581
391.152802	20130.302704	29.826599
391.806862	20148.276704	29.831616
391.984603	20187.546024	29.836634
392.209013	20205.643221	29.841652
392.658079	20236.511694	29.846669
392.718767	20278.152911	29.851687
393.527037	20306.824167	29.856704
393.525209	20338.675587	29.861722
394.530678	20356.530164	29.866740
394.551452	20389.934073	29.871757
394.728450	20419.946076	29.876775
395.355749	20438.859762	29.881792
395.423611	20474.107016	29.886810
395.994153	20509.184435	29.891828
396.368973	20530.793500	29.896845
396.684152	20569.098131	29.901863
397.070240	20600.163739	29.906880
397.165141	20637.752919	29.911898
397.557620	20666.648115	29.916916
397.976960	20705.504990	29.921933
398.199972	20737.398785	29.926951
398.855705	20778.132353	29.931968
399.281410	20805.272186	29.936986
399.785884	20846.188619	29.942004
400.303188	20889.720314	29.947021
400.511100	20916.850648	29.952039
401.167275	20950.057484	29.957056
401.454100	20990.586160	29.962074
402.250596	21013.191900	29.967092
402.542503	21058.008495	29.972109
402.688007	21093.084946	29.977127
403.236133	21126.368349	29.982144
403.330768	21161.968943	29.987162
403.889050	21199.845327	29.992180
404.267745	21229.035460	29.997197
404.593716	21267.153838	30.002215
405.096872	21306.736129	30.007232
405.246918	21351.874981	30.012250
405.636540	21374.102330	30.017268
406.520116	21419.340707	30.022285
406.847859	21451.425069	30.027303
407.450403	21483.785668	30.032320
407.859118	21534.946320	30.037338
408.193483	21557.481060	30.042356
408.749701	21584.286776	30.047373
408.843418	21633.751250	30.052391
409.654275	21652.552357	30.057408
409.730218	21694.426323	30.062426
410.251551	21729.027209	30.067444
410.675344	21764.226132	30.072461
411.052633	21798.447347	30.077479
411.585975	21827.805287	30.082496
411.903243	21874.340100	30.087514
412.578709	21904.598639	30.092532
412.620337	21938.855191	30.097549
412.619397	21971.762826	30.102567
413.538883	22004.524506	30.107584
413.715862	22040.512245	30.112602
414.102844	22085.790440	30.117620
415.040712	22111.969343	30.122637
415.339992	22151.248342	30.127655
415.611236	22183.300869	30.132672
416.019005	22228.894520	30.137690
416.273094	22258.972717	30.142708
416.694223	22291.360155	30.147725
416.708455	22347.790440	30.152743
417.894747	22377.017621	30.157760
418.101847	22415.164563	30.162778
418.283465	22449.406861	30.167796
418.816083	22488.689022	30.172813
418.974986	22536.891762	30.177831
419.565550	22564.458112	30.182848
420.381422	22602.593030	30.187866
420.691118	22634.417711	30.192884
421.116481	22665.521614	30.197901
421.508290	22697.761726	30.202919
422.095020	22721.880403	30.207936
422.360512	22759.949074	30.212954
422.520528	22785.374712	30.217972
422.917738	22816.787884	30.222989
423.275465	22854.322716	30.228007
423.831224	22887.816468	30.233024
424.316642	22921.922713	30.238042
424.740260	22952.489719	30.243060
425.086649	22991.545256	30.248077
425.388566	23034.050567	30.253095
426.011671	23056.623091	30.258112
426.452519	23088.102079	30.263130
426.572879	23128.865257	30.268148
427.105253	23154.654007	30.273165
427.484677	23199.606852	30.278183
428.189989	23232.855769	30.283200
428.370296	23264.308817	30.288218
428.790677	23308.588143	30.293236
428.992360	23339.621490	30.298253
429.907208	23390.899511	30.303271
430.343395	23427.539552	30.308288
430.696872	23466.424698	30.313306
430.903827	23503.380375	30.318324
431.368405	23536.488380	30.323341
431.869437	23585.973123	30.328359
432.253883	23619.818360	30.333376
432.593478	23658.485471	30.338394
433.408875	23701.596591	30.343412
433.767644	23738.068763	30.348429
433.824629	23771.446525	30.353447
434.639434	23820.260281	30.358464
435.259569	23845.947247	30.363482
435.194837	23890.797220	30.368500
435.988885	23926.954910	30.373517
436.275524	23969.785204	30.378535
436.700165	24006.202893	30.383552
437.189222	24048.763341	30.388570
437.305535	24091.196343	30.393588
438.261151	24132.888149	30.398605
438.548930	24168.562421	30.403623
439.199556	24202.262259	30.408640
439.748783	24253.890393	30.413658
439.726904	24289.597238	30.418676
440.826940	24326.367475	30.423693
440.688649	24353.032294	30.428711
441.271658	24394.884176	30.433728
441.393354	24430.927112	30.438746
442.101090	24476.581218	30.443764
442.575020	24521.624407	30.448781
442.518198	24564.718040	30.453799
443.132316	24608.359943	30.458816
443.709886	24645.359261	30.463834
444.172878	24691.637942	30.468852
444.711994	24730.000054	30.473869
445.070138	24777.050139	30.478887
445.396955	24817.217015	30.483904
445.890282	24858.463517	30.488922
446.382866	24908.671040	30.493940
447.283509	24937.505179	30.498957
447.556788	24978.709532	30.503975
447.864447	25019.936681	30.508992
448.453135	25052.266939	30.514010
449.124537	25099.149365	30.519028
449.137895	25132.619002	30.524045
449.637710	25171.247244	30.529063
449.609356	25206.212685	30.534080
450.373207	25257.540221	30.539098
450.484081	25303.916674	30.544116
451.408072	25333.217587	30.549133
451.702385	25384.607434	30.554151
452.506079	25412.029569	30.559168
452.976637	25444.805931	30.564186
453.091805	25481.003551	30.569204
453.542756	25514.874647	30.574221
453.868636	25551.532757	30.579239
454.553693	25595.666954	30.584256
454.963673	25624.160781	30.589274
455.207756	25671.415134	30.594292
455.829129	25710.056014	30.599309
455.975007	25750.242396	30.604327
456.714149	25803.723700	30.609344
457.031750	25841.585572	30.614362
457.108180	25891.719736	30.619380
457.828515	25928.464778	30.624397
458.107961	25973.143362	30.629415
458.676887	26020.445853	30.634432
459.331711	26060.059817	30.639450
459.631564	26114.589463	30.644468
460.382093	26151.005088	30.649485
460.676754	26199.176736	30.654503
460.892046	26246.585683	30.659520
462.017644	26292.967209	30.664538
462.061632	26333.108721	30.669556
462.402776	26379.440495	30.674573
463.024737	26434.659126	30.679591
463.550792	26476.762082	30.684608
464.060341	26526.930508	30.689626
464.501085	26578.873780	30.694644
465.224612	26603.957897	30.699661
465.683084	26648.709544	30.704679
466.247191	26691.844531	30.709696
466.570590	26730.704192	30.714714
467.028526	26773.396405	30.719732
467.043716	26817.685588	30.724749
467.841524	26866.933517	30.729767
468.396951	26912.199750	30.734784
468.869085	26956.410518	30.739802
469.026681	27009.080148	30.744820
469.757033	27041.920653	30.749837
469.740957	27098.890476	30.754855
470.733744	27139.715946	30.759872
471.561895	27187.622255	30.764890
471.882613	27238.874448	30.769908
472.209503	27278.539164	30.774925
472.490353	27334.722465	30.779943
473.214542	27369.889511	30.784960
473.589944	27412.477083	30.789978
474.197551	27463.931676	30.794996
474.510269	27497.416287	30.800013
475.184498	27547.219724	30.805031
475.616262	27595.069725	30.810048
476.159774	27632.371315	30.815066
476.355012	27683.979973	30.820084
477.093044	27724.899454	30.825101
477.303094	27770.215616	30.830119
478.020025	27817.851846	30.835136
478.691211	27846.388133	30.840154
478.697732	27895.662670	30.845172
479.427242	27938.000499	30.850189
479.911379	27979.584062	30.855207
480.286241	28020.138457	30.860224
480.735285	28056.538582	30.865242
481.169529	28107.531639	30.870260
481.856866	28147.589812	30.875277
482.446483	28200.128467	30.880295
482.721613	28234.630222	30.885312
483.358295	28273.902082	30.890330
483.945579	28314.475642	30.895348
484.326582	28354.692244	30.900365
484.564263	28389.017527	30.905383
484.996941	28430.888300	30.910400
485.492186	28465.581230	30.915418
485.837910	28520.722865	30.920436
486.312603	28560.019022	30.925453
487.030525	28611.812090	30.930471
487.002312	28643.844186	30.935488
487.882523	28689.591309	30.940506
488.044913	28740.467155	30.945524
488.523802	28782.208086	30.950541
489.220193	28832.421660	30.955559
489.493797	28890.519840	30.960576
490.379473	28923.051114	30.965594
490.436055	28980.425190	30.970612
491.549342	29024.030343	30.975629
491.970349	29070.662095	30.980647
492.040123	29124.999489	30.985664
492.628929	29160.116844	30.990682
493.091002	29214.247630	30.995700
493.663196	29257.113170	31.000717
494.092816	29300.936257	31.005735
494.240103	29353.119356	31.010752
494.964231	29397.165272	31.015770
495.638151	29458.603250	31.020788
496.194651	29513.747843	31.025805
496.519003	29562.933470	31.030823
497.167351	29619.473458	31.035840
497.593269	29651.971746	31.040858
498.143721	29711.812547	31.045876
498.540651	29770.006815	31.050893
499.264857	29818.120553	31.055911
499.940604	29873.621989	31.060928
500.515096	29918.959136	31.065946
500.770042	29968.580156	31.070964
501.332660	30014.323356	31.075981
501.613691	30072.077169	31.080999
502.140271	30125.095829	31.086016
502.637095	30172.670791	31.091034
503.467643	30229.832538	31.096052
504.063467	30277.568086	31.101069
504.644879	30322.198393	31.106087
505.018750	30370.422097	31.111104
505.594078	30409.084199	31.116122
505.805622	30457.476982	31.121140
506.640230	30505.473372	31.126157
507.449926	30546.927135	31.131175
507.568162	30595.815316	31.136192
508.137763	30634.854324	31.141210
508.996283	30680.222160	31.146228
509.286171	30721.699246	31.151245
509.963787	30763.399391	31.156263
510.273381	30811.003906	31.161280
510.846458	30852.305077	31.166298
510.980072	30898.048996	31.171316
511.522892	30938.983065	31.176333
512.171437	30992.441660	31.181351
512.747075	31039.949132	31.186368
513.272616	31071.250357	31.191386
514.035076	31133.951094	31.196404
514.185716	31183.646436	31.201421
515.196810	31220.660597	31.206439
515.341097	31266.709762	31.211456
515.887970	31306.164201	31.216474
516.332782	31353.769892	31.221492
516.592090	31399.702558	31.226509
517.093295	31445.027366	31.231527
517.305684	31498.881504	31.236544
518.225778	31539.628329	31.241562
518.599730	31592.417925	31.246580
519.020594	31635.380567	31.251597
519.749283	31677.964224	31.256615
520.018792	31724.441916	31.261632
520.744542	31763.650060	31.266650
520.861311	31814.299379	31.271668
521.478052	31860.830410	31.276685
522.018614	31909.238990	31.281703
522.130495	31970.176057	31.286720
523.117185	32026.809780	31.291738
523.532112	32077.666102	31.296756
523.557469	32127.684584	31.301773
524.164668	32183.412893	31.306791
524.762665	32249.407497	31.311808
525.553049	32309.545576	31.316826
525.845975	32367.260747	31.321844
526.526396	32425.770272	31.326861
527.022113	32473.061313	31.331879
527.233992	32539.546873	31.336896
527.918325	32602.215252	31.341914
528.200413	32654.127049	31.346932
528.804692	32724.861939	31.351949
529.535041	32778.754165	31.356967
530.061282	32850.184058	31.361984
530.815865	32911.349336	31.367002
531.513127	32967.885645	31.372020
532.183012	33019.046429	31.377037
532.915835	33068.893694	31.382055
532.990174	33134.747876	31.387072
533.887093	33188.834675	31.392090
534.221212	33245.097459	31.397108
534.778854	33305.280573	31.402125
535.262975	33355.788294	31.407143
535.639672	33420.476410	31.412160
536.549772	33479.566746	31.417178
537.193737	33525.248765	31.422196
537.487909	33584.949424	31.427213
538.147177	33631.923006	31.432231
538.618680	33691.648327	31.437248
539.670080	33740.602192	31.442266
540.142253	33802.517822	31.447284
540.653890	33854.224722	31.452301
540.670807	33912.082080	31.457319
541.307107	33966.845507	31.462336
542.043402	34023.012638	31.467354
542.629517	34078.166554	31.472372
542.902452	34134.233983	31.477389
544.144557	34192.747890	31.482407
544.213365	34246.681432	31.487424
544.626482	34294.609505	31.492442
545.280240	34348.856820	31.497460
545.331636	34411.898216	31.502477
546.416529	34462.637864	31.507495
546.820516	34522.168843	31.512512
547.448933	34581.716535	31.517530
547.982771	34629.893777	31.522548
548.609459	34680.391118	31.527565
549.501554	34736.802958	31.532583
549.583062	34791.493443	31.537600
550.171628	34854.813595	31.542618
550.924687	34904.359670	31.547636
551.277976	34955.789830	31.552653
552.523927	35010.335649	31.557671
552.889810	35064.762154	31.562688
553.086961	35110.275989	31.567706
553.911813	35153.439051	31.572724
554.258591	35202.267344	31.577741
554.954007	35240.645526	31.582759
554.867067	35298.789634	31.587776
555.375467	35344.438764	31.592794
555.937143	35395.428580	31.597812
556.099673	35459.651377	31.602829
556.695157	35511.409146	31.607847
557.503669	35566.881156	31.612864
558.169090	35620.496026	31.617882
558.477632	35687.122453	31.622900
559.115921	35743.140761	31.627917
559.515331	35808.060961	31.632935
560.136449	35867.068122	31.637952
560.683394	35916.408073	31.642970
561.587605	35979.840916	31.647988
561.885742	36054.884540	31.653005
562.786007	36113.590676	31.658023
563.234364	36166.750733	31.663040
563.525159	36234.366823	31.668058
564.701724	36289.568700	31.673076
564.855871	36353.234268	31.678093
565.792638	36409.928018	31.683111
565.956141	36482.294021	31.688128
566.457268	36540.938184	31.693146
567.204542	36589.770245	31.698164
567.845295	36658.267404	31.703181
567.881515	36717.607676	31.708199
568.748389	36787.762797	31.713216
569.400037	36840.562950	31.718234
570.017475	36897.367876	31.723252
570.501362	36966.794841	31.728269
571.350747	37026.358236	31.733287
571.988515	37087.405571	31.738304
572.463617	37162.475003	31.743322
573.588480	37210.526632	31.748340
574.023363	37270.232005	31.753357
574.422020	37333.794276	31.758375
575.050876	37381.328725	31.763392
575.034934	37443.555412	31.768410
576.102149	37511.467593	31.773428
576.393479	37584.233475	31.778445
577.039831	37639.827055	31.783463
577.530263	37703.852047	31.788480
578.264852	37773.903456	31.793498
579.021617	37835.157719	31.798516
579.500183	37906.132635	31.803533
580.267359	37953.541532	31.808551
580.833900	38024.335062	31.813568
581.110002	38081.951399	31.818586
581.963250	38137.029330	31.823604
582.181554	38203.348499	31.828621
583.132754	38261.049406	31.833639
583.506628	38312.602483	31.838656
584.062785	38389.547987	31.843674
584.962730	38449.091897	31.848692
585.048840	38515.405663	31.853709
586.069249	38572.584749	31.858727
586.154391	38643.406667	31.863744
587.032816	38709.015553	31.868762
587.422728	38763.641734	31.873780
588.200866	38835.618678	31.878797
588.791118	38894.530303	31.883815
589.068966	38954.484977	31.888832
589.854568	39027.963984	31.893850
590.528361	39090.704014	31.898868
590.700709	39157.877065	31.903885
591.301607	39216.993147	31.908903
592.026511	39274.299081	31.913920
592.677948	39339.726818	31.918938
593.280568	39394.004021	31.923956
593.956441	39464.175798	31.928973
594.913154	39521.791388	31.933991
595.170608	39581.944046	31.939008
595.622914	39652.466047	31.944026
596.424976	39700.097833	31.949044
596.740881	39763.691718	31.954061
597.441310	39827.559975	31.959079
597.893108	39890.222670	31.964096
598.731185	39949.863775	31.969114
599.557888	40011.865071	31.974132
599.803013	40075.670622	31.979149
600.462919	40141.756429	31.984167
601.414061	40202.752858	31.989184
601.384712	40265.619552	31.994202
602.446531	40325.019664	31.999220
603.092991	40397.573810	32.004237
603.513132	40456.225005	32.009255
604.162597	40517.673311	32.014272
604.622483	40588.273407	32.019290
605.246220	40659.588534	32.024308
605.798043	40724.662010	32.029325
606.513156	40792.265800	32.034343
607.288938	40858.518107	32.039360
607.324882	40922.942070	32.044378
608.384609	40982.852916	32.049396
609.055507	41059.222369	32.054413
610.097807	41121.712628	32.059431
610.615354	41183.860569	32.064448
611.122481	41253.000022	32.069466
612.010114	41311.431366	32.074484
612.339872	41384.651089	32.079501
612.991037	41441.019393	32.084519
613.645067	41504.572805	32.089536
614.017206	41577.432690	32.094554
614.801375	41630.073193	32.099572
615.204469	41705.321507	32.104589
615.935472	41772.118041	32.109607
616.609685	41845.115268	32.114624
617.277749	41920.393230	32.119642
618.097600	41974.683131	32.124660
618.161723	42046.187743	32.129677
618.864062	42105.068987	32.134695
619.599146	42180.109600	32.139712
620.108370	42247.557023	32.144730
620.851724	42312.478104	32.149748
621.616780	42389.970886	32.154765
622.064215	42462.714441	32.159783
623.321500	42523.333216	32.164800
623.663610	42582.038780	32.169818
624.057790	42647.306105	32.174836
624.698143	42712.450843	32.179853
625.637523	42781.729694	32.184871
625.792620	42854.627334	32.189888
626.256316	42920.995473	32.194906
627.550715	42988.644035	32.199924
627.971057	43062.777306	32.204941
628.586033	43120.946883	32.209959
629.245204	43192.335342	32.214976
629.608697	43259.150657	32.219994
630.524346	43314.341089	32.225012
631.297578	43382.879271	32.230029
631.617022	43450.668708	32.235047
632.075626	43517.418693	32.240064
632.726741	43582.151070	32.245082
633.541792	43655.198395	32.250100
634.080537	43714.317021	32.255117
634.311795	43779.700507	32.260135
634.958606	43845.047045	32.265152
635.647753	43909.947922	32.270170
636.463143	43971.462294	32.275188
637.217805	44035.853892	32.280205
637.739022	44100.104356	32.285223
638.661475	44162.820430	32.290240
639.027725	44232.057392	32.295258
640.036441	44298.520227	32.300276
639.983074	44364.811680	32.305293
640.644355	44430.356788	32.310311
641.563468	44489.999076	32.315328
642.063921	44569.407617	32.320346
643.055313	44633.020075	32.325364
643.514978	44701.416030	32.330381
644.179371	44769.150004	32.335399
644.844187	44829.365915	32.340416
645.329107	44902.239051	32.345434
645.970708	44976.829554	32.350452
646.418424	45048.458993	32.355469
647.047027	45125.145744	32.360487
647.756007	45200.891158	32.365504
648.870130	45281.388457	32.370522
649.249811	45344.558245	32.375540
649.942623	45421.608185	32.380557
650.407945	45506.113533	32.385575
651.340767	45573.720733	32.390592
651.965663	45651.253347	32.395610
652.522544	45726.047134	32.400628
653.316553	45800.404110	32.405645
653.650868	45884.149696	32.410663
654.412174	45953.646559	32.415680
655.023611	46028.543039	32.420698
655.807491	46093.457876	32.425716
656.436171	46174.408756	32.430733
656.978244	46251.016498	32.435751
658.010774	46328.310768	32.440768
658.516201	46413.072472	32.445786
659.247328	46481.433119	32.450804
659.701262	46556.667214	32.455821
660.597876	46634.882058	32.460839
661.192218	46703.064027	32.465856
661.706664	46782.501656	32.470874
662.348336	46855.009009	32.475892
663.368779	46945.710069	32.480909
663.648699	47018.590529	32.485927
664.392183	47088.593457	32.490944
665.223999	47180.353182	32.495962
665.828100	47258.587405	32.500980
666.860819	47324.640064	32.505997
667.297656	47402.763598	32.511015
668.282206	47472.342778	32.516032
668.837990	47553.532653	32.521050
669.358760	47627.430385	32.526068
670.024850	47696.605149	32.531085
670.668073	47783.143943	32.536103
671.545253	47843.678534	32.541120
671.693969	47932.412579	32.546138
672.404964	48003.359042	32.551156
673.148617	48071.249608	32.556173
673.723749	48166.211516	32.561191
674.474974	48234.805677	32.566208
674.972888	48322.552104	32.571226
675.203212	48406.742864	32.576244
675.933923	48498.105609	32.581261
676.503228	48579.022836	32.586279
677.531557	48669.762368	32.591296
678.357934	48747.940650	32.596314
679.136173	48822.381519	32.601332
679.915399	48886.049656	32.606349
680.402920	48971.482602	32.611367
681.098543	49030.241286	32.616384
681.528517	49121.230379	32.621402
682.422863	49190.107480	32.626420
683.136161	49268.044446	32.631437
683.576073	49344.305657	32.636455
684.652325	49419.176449	32.641472
684.889627	49499.703990	32.646490
685.241053	49580.531985	32.651508
686.072314	49666.580728	32.656525
686.935164	49759.844759	32.661543
687.638321	49829.166369	32.666560
688.180759	49934.369400	32.671578
688.866273	50004.496803	32.676596
689.733696	50094.217911	32.681613
690.302092	50175.151475	32.686631
690.852917	50266.700824	32.691648
691.469953	50355.270654	32.696666
691.940073	50446.796303	32.701684
693.243920	50542.252663	32.706701
693.570387	50642.356328	32.711719
694.288732	50724.575026	32.716736
694.975165	50811.442470	32.721754
696.233151	50910.142620	32.726772
696.727106	50991.192985	32.731789
697.473389	51092.581411	32.736807
698.386211	51174.428713	32.741824
698.989226	51270.042500	32.746842
699.524860	51350.076696	32.751860
700.265437	51432.433698	32.756877
700.954472	51520.043014	32.761895
701.592433	51611.394772	32.766912
702.477271	51696.774029	32.771930
702.834065	51791.148664	32.776948
704.042056	51875.717150	32.781965
704.483882	51973.028877	32.786983
705.291773	52069.029654	32.792000
706.169299	52153.192829	32.797018
706.469226	52242.802949	32.802036
707.708890	52327.456603	32.807053
708.441841	52431.355998	32.812071
708.969581	52510.113773	32.817088
709.592742	52604.088163	32.822106
710.577842	52691.653765	32.827124
711.487102	52768.770025	32.832141
711.808799	52865.600644	32.837159
712.717894	52947.140117	32.842176
713.521811	53037.700316	32.847194
714.157090	53136.078822	32.852212
714.948389	53215.667709	32.857229
715.495431	53315.811784	32.862247
716.032625	53395.493978	32.867264
716.938536	53483.657477	32.872282
717.286430	53570.757475	32.877300
718.115951	53654.265332	32.882317
718.689893	53763.467374	32.887335
719.645136	53848.484244	32.892352
720.406973	53946.334101	32.897370
721.051359	54034.802379	32.902388
721.843554	54129.419521	32.907405
722.305950	54217.425901	32.912423
723.421968	54302.108540	32.917440
723.783962	54396.052566	32.922458
724.568146	54493.541298	32.927476
725.378693	54565.506210	32.932493
726.005024	54666.471743	32.937511
726.896698	54747.952063	32.942528
727.241885	54840.953218	32.947546
727.593724	54928.842049	32.952564
728.640976	55013.368515	32.957581
729.264681	55108.245684	32.962599
730.091563	55189.283605	32.967616
730.620310	55280.885330	32.972634
731.143760	55381.315489	32.977652
732.230880	55475.770235	32.982669
732.938235	55579.722068	32.987687
733.344676	55675.857400	32.992704
734.238774	55763.180004	32.997722
735.060718	55866.153930	33.002740
735.628006	55966.965243	33.007757
736.319008	56068.015676	33.012775
736.964284	56166.129585	33.017792
738.067977	56268.205936	33.022810
738.644347	56374.489994	33.027828
739.282114	56469.263912	33.032845
740.143973	56585.308932	33.037863
740.610534	56688.712398	33.042880
741.447231	56783.960428	33.047898
742.412441	56891.244523	33.052916
743.013903	56992.687279	33.057933
743.681977	57099.863665	33.062951
744.511494	57202.653663	33.067968
745.157654	57307.490358	33.072986
745.731179	57422.292484	33.078004
746.854613	57523.221874	33.083021
747.452483	57646.470182	33.088039
748.144900	57746.100691	33.093056
749.379085	57845.168123	33.098074
749.942454	57950.401037	33.103092
750.999038	58063.458591	33.108109
751.440064	58168.131488	33.113127
752.759608	58273.556988	33.118144
753.618061	58369.895918	33.123162
754.094507	58466.879901	33.128180
754.709659	58570.394876	33.133197
755.786280	58666.117728	33.138215
756.573501	58774.155452	33.143232
757.364879	58878.142113	33.148250
758.137627	58980.413414	33.153268
758.888815	59075.958209	33.158285
759.489889	59173.127204	33.163303
760.351645	59268.844217	33.168320
761.187650	59373.634988	33.173338
761.700711	59481.165690	33.178356
762.612382	59580.073801	33.183373
763.058402	59674.193029	33.188391
763.933875	59790.639809	33.193408
764.943243	59898.665753	33.198426
765.386425	59992.129638	33.203444
766.288919	60095.687047	33.208461
766.969405	60198.472726	33.213479
767.717772	60306.847380	33.218496
768.650885	60410.483491	33.223514
769.255501	60524.609199	33.228532
770.532099	60627.905190	33.233549
770.981833	60727.805420	33.238567
771.220609	60825.554194	33.243584
772.560881	60930.105255	33.248602
773.317891	61045.289454	33.253620
774.051456	61139.620711	33.258637
774.544125	61256.335129	33.263655
775.190988	61360.788195	33.268672
776.263232	61455.033285	33.273690
776.786964	61565.379545	33.278708
777.766114	61647.239957	33.283725
778.384293	61752.407673	33.288743
778.856096	61858.952762	33.293760
780.143765	61954.245353	33.298778
780.783388	62053.046126	33.303796
781.432770	62158.210761	33.308813
782.477731	62258.778499	33.313831
783.308591	62358.257038	33.318848
784.117283	62458.972290	33.323866
784.927511	62558.809179	33.328884
785.388850	62663.141540	33.333901
786.275380	62751.500613	33.338919
787.119746	62865.308941	33.343936
787.681251	62958.210553	33.348954
788.612853	63064.161188	33.353972
789.386288	63178.773107	33.358989
789.925257	63293.177921	33.364007
790.411081	63400.164821	33.369024
791.248930	63504.338019	33.374042
792.386624	63628.702639	33.379060
793.173164	63735.502467	33.384077
794.094045	63848.778894	33.389095
794.914177	63965.890675	33.394112
795.732286	64064.127925	33.399130
796.465622	64194.536490	33.404148
797.712890	64288.146104	33.409165
798.303021	64395.569709	33.414183
798.652433	64512.237750	33.419200
799.995017	64622.939028	33.424218
800.405218	64740.906848	33.429236
801.768116	64850.809464	33.434253
802.237203	64960.468558	33.439271
802.763602	65070.763557	33.444288
803.929971	65184.012979	33.449306
804.499639	65305.175350	33.454324
805.288269	65405.863993	33.459341
806.333606	65520.368000	33.464359
806.988923	65649.553185	33.469376
808.287185	65754.464375	33.474394
808.914899	65867.490504	33.479412
809.733553	65977.514360	33.484429
810.749951	66075.671397	33.489447
811.511395	66199.336004	33.494464
812.786779	66305.322154	33.499482
813.059993	66411.411376	33.504500
814.327561	66522.691473	33.509517
814.952078	66624.658569	33.514535
815.629285	66739.002526	33.519552
816.668500	66844.625843	33.524570
817.237595	66961.928707	33.529588
817.953637	67061.347572	33.534605
819.075657	67179.160806	33.539623
819.572204	67285.432449	33.544640
820.566979	67388.574854	33.549658
821.145284	67514.856995	33.554676
822.056648	67624.387307	33.559693
822.940825	67731.216676	33.564711
823.643523	67849.292677	33.569728
824.180659	67958.500943	33.574746
825.218189	68074.777808	33.579764
826.241837	68187.264060	33.584781
827.148908	68306.389967	33.589799
827.450930	68407.812037	33.594816
828.799107	68533.492396	33.599834
829.293157	68645.682987	33.604852
830.424974	68752.305831	33.609869
831.057303	68867.136596	33.614887
831.711086	68981.673582	33.619904
832.646799	69078.764078	33.624922
833.129366	69188.664236	33.629940
833.606793	69297.541499	33.634957
834.795803	69409.052106	33.639975
835.319619	69514.951022	33.644992
836.297411	69628.116389	33.650010
837.086247	69761.756009	33.655028
838.032632	69873.492539	33.660045
839.055948	69983.889075	33.665063
839.717145	70104.071071	33.670080
840.542736	70218.263791	33.675098
841.162918	70332.497415	33.680116
842.048474	70450.709343	33.685133
842.907714	70576.432015	33.690151
843.787658	70711.655957	33.695168
844.596506	70825.930558	33.700186
845.495199	70956.157482	33.705204
846.171660	71068.482366	33.710221
847.320973	71198.302546	33.715239
847.719605	71328.728250	33.720256
848.845940	71453.159813	33.725274
849.705990	71587.330187	33.730292
850.719927	71707.089706	33.735309
851.700025	71830.055254	33.740327
852.217435	71959.535542	33.745344
853.557031	72083.005880	33.750362
854.422395	72213.815038	33.755380
855.240836	72332.554283	33.760397
856.306224	72460.150974	33.765415
857.023137	72574.241341	33.770432
857.828965	72690.157859	33.775450
858.631475	72810.786878	33.780468
859.776234	72938.676803	33.785485
860.597069	73074.507100	33.790503
861.188770	73194.844264	33.795520
862.356468	73315.093154	33.800538
863.051961	73450.623997	33.805556
863.995201	73571.701940	33.810573
865.161212	73695.501061	33.815591
865.840350	73820.254150	33.820608
867.017406	73939.360247	33.825626
867.591393	74075.357757	33.830644
868.438685	74197.131734	33.835661
869.615380	74325.309098	33.840679
870.618396	74446.432592	33.845696
871.553434	74563.020720	33.850714
872.265378	74678.020973	33.855732
873.294755	74798.819504	33.860749
874.328780	74915.949692	33.865767
874.674773	75025.921026	33.870784
875.981500	75151.728967	33.875802
876.734721	75272.177317	33.880820
877.173068	75401.223051	33.885837
878.166086	75515.453855	33.890855
878.702792	75650.948645	33.895872
879.603775	75772.570669	33.900890
880.849432	75906.185160	33.905908
881.899009	76030.124214	33.910925
882.571441	76141.995176	33.915943
883.120291	76289.249856	33.920960
884.366159	76415.214208	33.925978
885.303854	76537.764136	33.930996
885.895944	76661.915208	33.936013
886.957205	76792.168987	33.941031
887.669596	76910.773431	33.946048
889.106801	77035.571139	33.951066
889.382476	77161.017055	33.956084
890.126813	77285.734671	33.961101
891.371407	77403.779333	33.966119
892.320570	77519.760832	33.971136
892.962085	77639.437199	33.976154
893.970045	77750.020995	33.981172
894.462745	77874.220557	33.986189
895.548300	77981.060685	33.991207
896.403778	78118.004259	33.996224
897.509661	78236.784715	34.001242
898.121038	78374.510309	34.006260
898.972437	78496.256622	34.011277
900.051250	78607.269399	34.016295
901.070745	78741.804908	34.021312
901.492688	78873.542885	34.026330
902.628872	79001.292181	34.031348
903.384767	79132.805653	34.036365
904.294877	79260.543202	34.041383
905.113136	79402.580361	34.046400
905.769455	79530.772589	34.051418
907.185944	79671.263886	34.056436
907.691716	79807.389950	34.061453
908.761304	79938.805633	34.066471
909.551006	80086.956378	34.071488
910.603411	80225.031529	34.076506
911.574826	80364.632851	34.081524
912.335667	80512.449539	34.086541
913.195432	80654.430754	34.091559
913.996840	80798.187518	34.096576
914.941639	80945.527440	34.101594
915.978971	81077.960928	34.106612
916.586030	81228.281277	34.111629
917.658562	81364.632935	34.116647
919.073947	81523.640511	34.121664
919.852254	81666.457610	34.126682
920.847415	81801.034284	34.131700
921.419922	81953.958980	34.136717
922.732142	82103.156225	34.141735
923.429653	82247.458074	34.146752
924.369764	82393.334007	34.151770
925.483385	82538.138269	34.156788
926.135236	82690.396777	34.161805
927.102617	82827.369246	34.166823
927.921349	82977.140940	34.171840
928.984484	83129.859465	34.176858
930.457248	83276.563981	34.181876
931.252506	83419.604292	34.186893
932.134175	83566.965175	34.191911
932.873655	83711.319871	34.196928
933.718829	83850.419192	34.201946
935.103246	84002.463979	34.206964
935.884665	84150.718295	34.211981
937.186259	84289.510672	34.216999
938.056514	84441.314351	34.222016
939.003525	84575.997446	34.227034
939.920803	84712.767915	34.232052
940.593120	84857.128192	34.237069
941.425476	85004.734145	34.242087
942.262529	85157.174393	34.247104
943.438805	85300.890941	34.252122
944.839386	85436.839099	34.257140
945.918406	85586.356806	34.262157
947.094643	85729.854537	34.267175
947.373089	85863.402767	34.272192
948.212975	86011.684561	34.277210
949.417157	86151.592486	34.282228
949.941565	86299.004424	34.287245
951.083364	86445.340719	34.292263
952.129752	86585.441844	34.297280
953.152011	86721.061365	34.302298
953.999427	86848.845048	34.307316
954.726933	86983.850398	34.312333
955.607926	87110.402334	34.317351
956.447821	87250.244148	34.322368
957.234557	87397.834732	34.327386
958.442462	87537.503487	34.332404
959.187728	87672.655382	34.337421
960.135367	87819.500588	34.342439
960.926619	87964.448804	34.347456
962.074126	88115.895008	34.352474
963.232632	88262.796685	34.357492
963.722095	88416.410299	34.362509
964.815078	88564.065081	34.367527
965.839776	88708.631175	34.372544
966.694093	88857.580258	34.377562
967.824049	89013.876306	34.382580
968.386407	89181.031982	34.387597
969.776535	89327.072890	34.392615
970.615878	89481.186084	34.397632
971.290121	89633.593533	34.402650
972.427049	89803.917778	34.407668
973.228459	89969.982547	34.412685
974.466611	90128.008369	34.417703
975.818235	90271.529909	34.422720
976.505685	90439.490082	34.427738
977.801597	90586.541536	34.432756
978.664368	90755.747022	34.437773
979.830202	90906.897750	34.442791
980.646235	91070.676617	34.447808
981.641077	91225.041088	34.452826
982.592849	91372.742838	34.457844
983.737016	91548.989563	34.462861
984.940269	91692.183330	34.467879
986.048078	91855.381280	34.472896
986.918986	92022.037283	34.477914
988.161175	92172.594667	34.482932
988.935618	92333.540770	34.487949
989.932321	92474.184613	34.492967
990.858973	92641.823019	34.497984
991.666219	92800.405917	34.503002
993.136697	92956.310411	34.508020
994.039898	93118.531611	34.513037
995.309061	93260.147651	34.518055
996.192079	93409.822628	34.523072
996.999694	93580.082279	34.528090
998.542448	93723.035615	34.533108
999.342762	93877.911121	34.538125
1000.122521	94032.417546	34.543143
1001.124478	94179.811499	34.548160
1002.110190	94345.173064	34.553178
1003.403513	94501.293905	34.558196
1004.509588	94658.187295	34.563213
1005.308667	94810.252055	34.568231
1006.541687	94949.668319	34.573248
1007.143362	95115.484670	34.578266
1008.132570	95276.572793	34.583284
1009.144628	95431.682563	34.588301
1010.384538	95586.774619	34.593319
1011.325396	95746.962248	34.598336
1011.925239	95903.795304	34.603354
1013.198505	96063.164047	34.608372
1013.938833	96226.439106	34.613389
1014.974001	96389.425929	34.618407
1016.009274	96551.141390	34.623424
1017.002537	96710.187071	34.628442
1018.039384	96867.454025	34.633460
1018.748199	97031.271309	34.638477
1019.576073	97191.562852	34.643495
1020.826097	97344.537090	34.648512
1021.636990	97499.053575	34.653530
1022.817555	97651.015602	34.658548
1023.541592	97808.890943	34.663565
1024.375761	97984.392857	34.668583
1025.505228	98134.397386	34.673600
1026.256569	98304.426428	34.678618
1027.333831	98458.151378	34.683636
1028.634977	98632.029515	34.688653
1029.521395	98799.241284	34.693671
1030.553883	98967.417638	34.698688
1031.734109	99135.722624	34.703706
1032.819388	99305.677843	34.708724
1033.770429	99481.702615	34.713741
1034.935745	99652.583923	34.718759
1035.924405	99809.174396	34.723776
1036.915568	99987.810816	34.728794
1037.962040	100153.251260	34.733812
1038.722374	100336.948998	34.738829
1039.739913	100509.905495	34.743847
1040.928204	100681.505329	34.748864
1041.886765	100868.358803	34.753882
1043.131832	101045.574025	34.758900
1044.300554	101224.563263	34.763917
1045.167861	101406.357828	34.768935
1046.085703	101588.525216	34.773952
1047.321443	101766.848647	34.778970
1048.579066	101944.523854	34.783988
1049.818825	102135.962184	34.789005
1050.804229	102302.692896	34.794023
1051.854278	102489.017433	34.799040
1052.708951	102665.314209	34.804058
1054.188346	102839.900574	34.809076
1055.332396	103017.817197	34.814093
1056.088196	103202.992421	34.819111
1057.202833	103358.424846	34.824128
1058.075629	103555.208915	34.829146
1058.999925	103728.848211	34.834164
1060.428893	103915.348249	34.839181
1061.226997	104096.964106	34.844199
1062.670692	104277.309336	34.849216
1063.881179	104474.449738	34.854234
1064.933700	104652.037990	34.859252
1066.060314	104823.523394	34.864269
1066.763608	105015.812413	34.869287
1068.046964	105192.618909	34.874304
1068.916418	105372.825946	34.879322
1070.113430	105557.564858	34.884340
1071.289908	105737.888266	34.889357
1072.659365	105928.883240	34.894375
1073.418604	106105.541842	34.899392
1074.486620	106289.205279	34.904410
1075.540924	106465.412187	34.909428
1076.770885	106652.065773	34.914445
1077.620595	106838.036249	34.919463
1078.912348	107016.145406	34.924480
1080.197840	107201.109082	34.929498
1080.856851	107382.289129	34.934516
1082.052460	107564.166984	34.939533
1083.129513	107753.171436	34.944551
1084.423387	107929.905691	34.949568
1085.344642	108120.927099	34.954586
1086.661752	108299.876564	34.959604
1087.816714	108474.484053	34.964621
1088.759067	108652.269155	34.969639
1089.820140	108836.913845	34.974656
1090.924413	109016.219911	34.979674
1091.956938	109194.310334	34.984692
1093.061728	109347.258651	34.989709
1093.871345	109523.589373	34.994727
1095.392366	109686.680450	34.999744
1096.039575	109869.082492	35.004762
1096.995094	110037.513398	35.009780
1098.228279	110208.559590	35.014797
1098.923086	110387.397686	35.019815
1099.896886	110571.815221	35.024832
1101.105482	110763.542414	35.029850
1102.051770	110933.411804	35.034868
1103.145377	111131.747798	35.039885
1104.110503	111322.290363	35.044903
1105.112786	111509.749781	35.049920
1106.270766	111714.514669	35.054938
1107.540440	111903.503397	35.059956
1108.476002	112105.901003	35.064973
1109.380857	112306.037528	35.069991
1110.753309	112505.794148	35.075008
1111.573255	112702.020347	35.080026
1112.624253	112907.242463	35.085044
1114.063138	113108.715365	35.090061
1115.356811	113312.088715	35.095079
1116.589214	113512.724523	35.100096
1117.602570	113719.656469	35.105114
1118.497585	113923.556256	35.110132
1119.990966	114124.571382	35.115149
1120.945933	114338.384241	35.120167
1122.394872	114536.064969	35.125184
1123.778785	114733.086353	35.130202
1124.641816	114938.151702	35.135220
1125.829940	115147.725864	35.140237
1126.989347	115356.280078	35.145255
1128.597012	115550.495498	35.150272
1129.310501	115747.330708	35.155290
1130.743338	115955.083925	35.160308
1131.757860	116149.806943	35.165325
1132.723434	116356.018563	35.170343
1133.758744	116554.022480	35.175360
1135.255004	116759.338382	35.180378
1136.218291	116961.664950	35.185396
1137.679973	117164.987548	35.190413
1138.587361	117367.833044	35.195431
1139.855874	117568.478920	35.200448
1141.068527	117772.303129	35.205466
1142.160710	117970.598846	35.210484
1143.945524	118162.914759	35.215501
1144.536197	118368.315835	35.220519
1145.462915	118579.909693	35.225536
1146.820870	118780.308448	35.230554
1147.823677	118983.643692	35.235572
1149.010020	119188.179143	35.240589
1150.077958	119400.984760	35.245607
1150.963446	119606.307830	35.250624
1152.364919	119802.980978	35.255642
1153.514267	120018.349987	35.260660
1154.725470	120219.087014	35.265677
1155.655168	120438.791185	35.270695
1156.795749	120638.744421	35.275712
1158.108719	120851.507394	35.280730
1159.207456	121068.970699	35.285748
1161.187803	121274.251156	35.290765
1161.729392	121482.850281	35.295783
1163.070044	121680.230343	35.300800
1164.053340	121894.677401	35.305818
1165.090879	122099.764605	35.310836
1166.426359	122302.218725	35.315853
1167.443968	122508.465260	35.320871
1168.748003	122709.381257	35.325888
1169.609107	122901.171216	35.330906
1170.641150	123100.436619	35.335924
1172.028632	123295.551152	35.340941
1172.670917	123494.959645	35.345959
1173.600837	123695.563900	35.350976
1174.905956	123903.914303	35.355994
1176.411493	124113.791858	35.361012
1177.812266	124311.813019	35.366029
1178.709902	124530.792225	35.371047
1179.722250	124730.933477	35.376064
1181.302788	124943.187058	35.381082
1181.995292	125158.427889	35.386100
1183.291441	125361.213256	35.391117
1184.409505	125576.906330	35.396135
1185.581595	125797.953193	35.401152
1186.918195	126001.243094	35.406170
1187.832398	126232.145640	35.411188
1189.466077	126456.112108	35.416205
1190.672072	126679.327059	35.421223
1191.968824	126879.067799	35.426240
1193.068030	127109.464708	35.431258
1194.373169	127319.093229	35.436276
1195.863190	127532.786612	35.441293
1196.813874	127748.814105	35.446311
1198.096525	127969.921647	35.451328
1199.530000	128187.444095	35.456346
1200.309371	128396.558392	35.461364
1201.455008	128611.710401	35.466381
1202.817938	128838.844315	35.471399
1204.357332	129063.783186	35.476416
1205.655079	129276.493586	35.481434
1206.377418	129497.311608	35.486452
1208.071031	129711.886228	35.491469
1209.112332	129942.998120	35.496487
1210.254056	130167.237383	35.501504
1211.395486	130387.599399	35.506522
1212.325372	130614.500797	35.511540
1213.817022	130838.129210	35.516557
1215.120575	131074.935679	35.521575
1216.166195	131296.371971	35.526592
1217.614229	131520.291265	35.531610
1218.829494	131760.578110	35.536628
1220.155406	131966.469184	35.541645
1221.450409	132202.423398	35.546663
1222.970559	132426.780792	35.551680
1224.229265	132657.052411	35.556698
1225.361605	132878.104970	35.561716
1226.767046	133089.517285	35.566733
1227.836026	133312.713050	35.571751
1228.724975	133545.587561	35.576768
1230.408707	133767.569229	35.581786
1231.100058	133993.215442	35.586804
1232.954623	134219.355530	35.591821
1234.135505	134437.000392	35.596839
1235.181938	134669.223007	35.601856
1236.494649	134880.560848	35.606874
1237.938147	135115.193167	35.611892
1238.885094	135334.746307	35.616909
1240.240537	135550.784938	35.621927
1241.449535	135777.004426	35.626944
1242.593025	135997.112676	35.631962
1243.832713	136235.095669	35.636980
1245.081054	136451.550908	35.641997
1246.403328	136685.162082	35.647015
1247.807467	136897.968405	35.652032
1249.046364	137118.423303	35.657050
1249.653165	137353.843682	35.662068
1250.933454	137560.525473	35.667085
1252.398116	137782.988721	35.672103
1253.217413	137990.865104	35.677120
1254.463701	138205.011749	35.682138
1255.648271	138437.339253	35.687156
1256.880897	138659.364823	35.692173
1258.130795	138891.304263	35.697191
1259.299567	139114.357715	35.702208
1260.307016	139343.436717	35.707226
1261.304171	139578.402308	35.712244
1262.677419	139808.349580	35.717261
1264.366818	140053.018114	35.722279
1265.533458	140280.745701	35.727296
1266.399428	140519.644834	35.732314
1267.397683	140768.997495	35.737332
1268.943811	141003.641175	35.742349
1269.850217	141250.717385	35.747367
1271.200596	141496.479298	35.752384
1272.648393	141760.068214	35.757402
1274.035936	142012.383416	35.762420
1275.118600	142263.913914	35.767437
1276.236157	142525.331407	35.772455
1277.595253	142778.785424	35.777472
1278.830241	143037.448269	35.782490
1280.051490	143295.734855	35.787508
1281.128520	143557.318888	35.792525
1282.637953	143825.529047	35.797543
1283.822100	144092.197161	35.802560
1285.144861	144347.507223	35.807578
1286.280492	144623.723726	35.812596
1287.626484	144889.825757	35.817613
1289.489429	145177.174867	35.822631
1290.390137	145437.191276	35.827648
1292.282427	145697.286629	35.832666
1293.180338	145962.291256	35.837684
1294.717034	146225.784542	35.842701
1296.210937	146499.584701	35.847719
1297.458928	146771.094042	35.852736
1298.639857	147036.402160	35.857754
1299.848131	147303.280305	35.862772
1300.942544	147576.165355	35.867789
1302.338221	147856.548784	35.872807
1303.362443	148131.478777	35.877824
1304.836843	148401.339400	35.882842
1305.996833	148681.755381	35.887860
1307.613143	148962.034650	35.892877
1309.144241	149243.928187	35.897895
1310.331499	149525.068965	35.902912
1312.042885	149794.317122	35.907930
1313.230411	150057.210660	35.912948
1314.464046	150328.685105	35.917965
1316.178774	150599.612707	35.922983
1317.363649	150884.898902	35.928000
1318.748879	151153.272112	35.933018
1319.759236	151432.883610	35.938036
1321.015237	151706.038515	35.943053
1322.435749	151975.895721	35.948071
1323.735302	152255.947456	35.953088
1325.357490	152531.280142	35.958106
1325.925066	152810.492907	35.963124
1327.553882	153092.297491	35.968141
1328.952247	153367.482886	35.973159
1330.192483	153651.309174	35.978176
1331.955705	153923.343190	35.983194
1332.860975	154213.368304	35.988212
1334.455944	154484.089465	35.993229
1336.138759	154763.144645	35.998247
1336.929273	155035.486705	36.003264
1338.910644	155289.633719	36.008282
1339.733452	155545.458011	36.013300
1341.071402	155800.247429	36.018317
1342.587757	156060.780821	36.023335
1343.513244	156333.223682	36.028352
1345.207351	156578.089988	36.033370
1346.153826	156856.977183	36.038388
1347.238221	157118.235839	36.043405
1348.729931	157396.516567	36.048423
1349.526466	157670.943445	36.053440
1351.081006	157946.858026	36.058458
1352.491848	158234.317126	36.063476
1353.829951	158509.675068	36.068493
1355.202962	158795.457140	36.073511
1356.296629	159085.537280	36.078528
1358.063145	159377.297051	36.083546
1359.041577	159663.607104	36.088564
1360.289568	159954.822347	36.093581
1362.065128	160241.474077	36.098599
1363.128407	160549.064404	36.103616
1364.673987	160832.992525	36.108634
1365.910900	161129.292566	36.113652
1367.181855	161424.954731	36.118669
1368.881080	161728.160449	36.123687
1370.270155	162026.002190	36.128704
1371.769747	162326.149537	36.133722
1372.670787	162630.394445	36.138740
1374.122969	162925.161747	36.143757
1375.835412	163220.243330	36.148775
1377.172490	163538.772254	36.153792
1378.633936	163832.275524	36.158810
1380.187489	164140.635667	36.163828
1381.762613	164434.466826	36.168845
1383.169476	164740.279852	36.173863
1384.336190	165040.412406	36.178880
1386.053603	165345.353643	36.183898
1387.202592	165650.390946	36.188916
1388.461873	165955.957742	36.193933
1390.380248	166257.890363	36.198951
1391.623596	166570.797956	36.203968
1393.156837	166863.078970	36.208986
1394.224783	167160.717285	36.214004
1395.706189	167472.043868	36.219021
1397.241293	167775.115998	36.224039
1398.578905	168087.079683	36.229056
1399.964102	168386.945035	36.234074
1401.631226	168696.447569	36.239092
1402.782888	169001.253577	36.244109
1404.543998	169298.334662	36.249127
1405.986508	169609.542823	36.254144
1407.371267	169903.911070	36.259162
1408.682774	170213.444592	36.264180
1410.314914	170520.427354	36.269197
1411.748291	170815.250211	36.274215
1413.196019	171116.595108	36.279232
1414.458034	171415.003219	36.284250
1415.871323	171725.088351	36.289268
1417.170658	172023.557621	36.294285
1419.074683	172325.494774	36.299303
1420.242053	172627.631731	36.304320
1421.207999	172926.555193	36.309338
1423.250697	173236.863495	36.314356
1424.404278	173539.884155	36.319373
1426.190859	173843.525486	36.324391
1427.088914	174158.572106	36.329408
1428.613281	174453.301063	36.334426
1430.106321	174758.367247	36.339444
1431.613750	175058.343952	36.344461
1432.950474	175340.393100	36.349479
1433.789457	175634.722137	36.354496
1435.444659	175929.717594	36.359514
1437.000809	176219.451680	36.364532
1438.054833	176512.011734	36.369549
1439.700953	176792.736252	36.374567
1440.996013	177108.434229	36.379584
1442.328584	177402.742960	36.384602
1444.099503	177703.872461	36.389620
1444.933652	178007.646104	36.394637
1446.821277	178306.196216	36.399655
1448.050648	178622.802946	36.404672
1449.612305	178926.880697	36.409690
1450.781878	179239.871279	36.414708
1452.174100	179553.080814	36.419725
1453.663438	179858.787908	36.424743
1455.094488	180186.882616	36.429760
1456.648613	180513.067921	36.434778
1458.363832	180829.569832	36.439796
1459.387398	181153.168730	36.444813
1461.285464	181469.606205	36.449831
1462.462308	181797.549917	36.454848
1463.724540	182118.754481	36.459866
1465.269448	182440.028503	36.464884
1466.722546	182784.648854	36.469901
1468.194117	183106.129373	36.474919
1469.894289	183448.898073	36.479936
1471.336279	183785.568205	36.484954
1472.666945	184116.343854	36.489972
1473.823113	184458.916854	36.494989
1475.844053	184796.843009	36.500007
1477.445926	185140.019332	36.505024
1478.862195	185487.645733	36.510042
1480.378314	185824.074886	36.515060
1481.643746	186159.747790	36.520077
1483.468964	186492.245657	36.525095
1484.936025	186839.008862	36.530112
1486.509131	187183.636806	36.535130
1488.056234	187518.496891	36.540148
1489.361536	187850.542760	36.545165
1491.106134	188188.534890	36.550183
1492.521835	188543.009414	36.555200
1494.369003	188881.559861	36.560218
1496.050888	189212.091466	36.565236
1497.634760	189555.640039	36.570253
1498.961985	189881.257851	36.575271
1500.651774	190221.758844	36.580288
1502.057185	190551.988166	36.585306
1503.353793	190878.301979	36.590324
1504.995962	191228.705601	36.595341
1506.694821	191560.301064	36.600359
1508.120891	191898.785875	36.605376
1509.701460	192235.799822	36.610394
1511.001296	192568.355317	36.615412
1512.619410	192902.561136	36.620429
1514.216322	193244.681256	36.625447
1515.894461	193589.113032	36.630464
1517.394975	193930.910063	36.635482
1518.888295	194263.214101	36.640500
1520.565507	194608.692605	36.645517
1522.064267	194928.481659	36.650535
1523.636001	195260.333600	36.655552
1525.190129	195594.386481	36.660570
1526.972665	195912.114947	36.665588
1528.204006	196250.934588	36.670605
1529.906440	196576.068372	36.675623
1531.536158	196909.214098	36.680640
1532.774052	197237.804965	36.685658
1534.444856	197544.095460	36.690676
1535.619714	197863.787327	36.695693
1537.468926	198169.911551	36.700711
1538.867575	198490.915193	36.705728
1540.233732	198795.585835	36.710746
1541.598863	199110.161012	36.715764
1542.778284	199430.799018	36.720781
1544.614703	199747.190978	36.725799
1545.967303	200090.313933	36.730816
1547.798301	200411.801045	36.735834
1549.259063	200735.382235	36.740852
1550.526528	201067.135312	36.745869
1551.964747	201393.732312	36.750887
1553.230557	201735.112781	36.755904
1554.846563	202084.918407	36.760922
1556.638961	202414.762676	36.765940
1558.078514	202754.684525	36.770957
1559.790599	203105.329877	36.775975
1561.127992	203446.389135	36.780992
1562.740386	203805.104139	36.786010
1564.107208	204143.952461	36.791028
1565.629806	204507.586734	36.796045
1567.421654	204854.125971	36.801063
1568.803468	205212.162040	36.806080
1570.336443	205569.387579	36.811098
1571.835669	205927.166337	36.816116
1572.935767	206304.020709	36.821133
1574.785354	206666.404932	36.826151
1576.620112	207041.211458	36.831168
1577.799719	207409.741110	36.836186
1579.929809	207776.820273	36.841204
1581.651309	208157.034556	36.846221
1583.247268	208523.303825	36.851239
1584.755378	208895.988954	36.856256
1586.351664	209276.025976	36.861274
1588.115476	209640.469395	36.866292
1589.615276	210018.240123	36.871309
1591.286701	210391.031955	36.876327
1593.033721	210758.733698	36.881344
1594.264739	211143.410823	36.886362
1595.992926	211511.118905	36.891380
1597.521594	211887.724899	36.896397
1599.405144	212266.889740	36.901415
1601.001725	212637.519519	36.906432
1602.429213	213031.645480	36.911450
1604.127009	213403.760134	36.916468
1605.735935	213782.545036	36.921485
1607.476651	214162.579600	36.926503
1609.372486	214540.761503	36.931520
1610.435493	214920.860354	36.936538
1612.322459	215298.030903	36.941556
1614.122660	215688.474839	36.946573
1615.756194	216058.832934	36.951591
1617.428353	216434.443420	36.956608
1619.207315	216821.619157	36.961626
1621.022370	217192.840526	36.966644
1622.610706	217571.872560	36.971661
1624.461475	217938.950936	36.976679
1625.899343	218310.162588	36.981696
1627.584754	218683.544363	36.986714
1629.347072	219061.791299	36.991732
1630.874754	219419.429361	36.996749
1632.752580	219801.495091	37.001767
1634.261717	220156.776660	37.006784
1635.978179	220545.119820	37.011802
1637.522861	220902.963279	37.016820
1639.052303	221284.456894	37.021837
1640.437694	221641.084541	37.026855
1642.357678	221993.510362	37.031872
1643.697396	222357.970795	37.036890
1645.265502	222720.972314	37.041908
1646.555186	223129.282719	37.046925
1648.012789	223484.685091	37.051943
1649.896160	223858.204302	37.056960
1651.337603	224216.151522	37.061978
1653.146809	224576.223444	37.066996
1654.561543	224952.820678	37.072013
1656.396471	225321.424905	37.077031
1657.960000	225699.473054	37.082048
1659.317351	226080.756816	37.087066
1660.832999	226448.655130	37.092084
1662.415358	226838.616243	37.097101
1663.860188	227224.232412	37.102119
1665.563014	227607.749677	37.107136
1666.859391	228000.326943	37.112154
1668.927474	228403.395284	37.117172
1669.995046	228807.392116	37.122189
1671.778915	229215.132709	37.127207
1673.549666	229625.619939	37.132224
1675.042737	230034.731791	37.137242
1676.808044	230437.271822	37.142260
1678.460137	230854.488002	37.147277
1680.153559	231278.734613	37.152295
1681.939163	231696.540729	37.157312
1683.315429	232126.354144	37.162330
1685.227910	232536.826066	37.167348
1687.223951	232971.924493	37.172365
1688.766038	233390.867636	37.177383
1690.713955	233821.099252	37.182400
1692.120943	234256.527039	37.187418
1693.832273	234673.692780	37.192436
1695.838264	235106.712266	37.197453
1697.403834	235542.371148	37.202471
1699.669916	235964.173055	37.207488
1700.880182	236385.718519	37.212506
1702.705445	236823.369734	37.217524
1704.608767	237257.274996	37.222541
1706.166059	237692.381486	37.227559
1708.320629	238115.654556	37.232576
1709.858007	238544.949153	37.237594
1711.819015	238978.442232	37.242612
1713.425288	239406.406332	37.247629
1714.731983	239842.828908	37.252647
1716.623069	240280.400540	37.257664
1718.031363	240716.223808	37.262682
1719.885017	241149.434106	37.267700
1721.998128	241592.661703	37.272717
1723.426418	242034.428281	37.277735
1725.289805	242469.798558	37.282752
1726.742828	242915.576200	37.287770
1728.700532	243359.797892	37.292788
1730.692541	243800.585298	37.297805
1732.104289	244245.965523	37.302823
1733.843863	244678.362316	37.307840
1735.771662	245129.272659	37.312858
1737.314855	245574.125127	37.317876
1738.910880	246020.112624	37.322893
1740.557601	246460.021077	37.327911
1742.648716	246901.761919	37.332928
1744.292775	247350.867795	37.337946
1746.163122	247803.620277	37.342964
1748.012211	248242.227352	37.347981
1749.761030	248692.409841	37.352999
1751.795829	249121.562683	37.358016
1753.362469	249570.734673	37.363034
1755.253518	249996.939949	37.368052
1756.999926	250431.476309	37.373069
1758.839470	250852.330783	37.378087
1760.700988	251256.187261	37.383104
1762.486109	251673.571129	37.388122
1764.423225	252082.928187	37.393140
1766.180906	252499.936105	37.398157
1767.783589	252915.521899	37.403175
1769.533041	253324.351837	37.408192
1771.289996	253739.938010	37.413210
1772.966534	254156.579203	37.418228
1774.830736	254582.461777	37.423245
1776.487642	255016.380794	37.428263
1778.024040	255431.521454	37.433280
1779.991579	255870.241495	37.438298
1781.589712	256302.417820	37.443316
1783.586916	256724.697261	37.448333
1784.845406	257172.400476	37.453351
1786.834896	257607.103552	37.458368
1788.308027	258049.512946	37.463386
1789.992814	258496.104357	37.468404
1791.634499	258946.538788	37.473421
1793.448671	259409.214508	37.478439
1795.353389	259848.986856	37.483456
1797.274440	260315.455310	37.488474
1798.955166	260768.067762	37.493492
1800.835088	261235.025463	37.498509
1802.162928	261704.843160	37.503527
1804.165725	262168.528639	37.508544
1805.773584	262644.802959	37.513562
1807.477968	263113.059089	37.518580
1809.777512	263581.953375	37.523597
1811.350410	264073.779484	37.528615
1813.234252	264542.818055	37.533632
1815.046861	265026.195459	37.538650
1816.838127	265506.883284	37.543668
1818.870519	265988.928065	37.548685
1820.652633	266478.279049	37.553703
1822.316858	266962.644630	37.558720
1824.067396	267454.641795	37.563738
1825.969174	267946.029185	37.568756
1828.106867	268428.638427	37.573773
1829.669900	268918.734277	37.578791
1831.808159	269402.307575	37.583808
1833.340574	269892.585063	37.588826
1835.325699	270398.892540	37.593844
1837.410329	270879.805411	37.598861
1839.054705	271382.712904	37.603879
1841.191949	271870.423569	37.608896
1843.182271	272361.612492	37.613914
1845.023197	272850.869267	37.618932
1847.153990	273333.980703	37.623949
1848.630402	273831.577225	37.628967
1850.883885	274314.768268	37.633984
1853.039117	274804.325258	37.639002
1854.616146	275295.958172	37.644020
1856.591394	275781.859601	37.649037
1858.400746	276266.822142	37.654055
1860.558799	276751.878493	37.659072
1862.166359	277235.449768	37.664090
1864.114581	277723.840932	37.669108
1866.243185	278189.948944	37.674125
1867.847658	278688.784099	37.679143
1869.790353	279169.221941	37.684160
1871.888168	279654.814994	37.689178
1873.846625	280135.044650	37.694196
1875.904519	280617.390417	37.699213
1877.599282	281097.457936	37.704231
1879.573799	281564.726353	37.709248
1881.670010	282024.708588	37.714266
1882.877223	282469.646303	37.719284
1884.957606	282927.113994	37.724301
1886.692878	283375.696138	37.729319
1888.420964	283828.545668	37.734336
1890.316962	284293.762010	37.739354
1892.277891	284762.217616	37.744372
1894.080308	285215.381130	37.749389
1895.652479	285696.446242	37.754407
1897.544749	286159.600100	37.759424
1899.334977	286634.606158	37.764442
1900.963823	287105.547791	37.769460
1903.278699	287578.381241	37.774477
1905.047394	288066.365852	37.779495
1906.853034	288548.576725	37.784512
1908.609478	289034.223072	37.789530
1910.753334	289524.350343	37.794548
1912.731798	290006.603633	37.799565
1914.598960	290512.673436	37.804583
1916.737009	290990.604068	37.809600
1918.436554	291486.309053	37.814618
1920.117288	291989.736711	37.819636
1922.230075	292491.795564	37.824653
1923.904776	293004.033712	37.829671
1926.206880	293498.767382	37.834688
1927.685220	294019.161380	37.839706
1929.219628	294526.386940	37.844724
1931.869859	295042.747478	37.849741
1933.574938	295564.443108	37.854759
1935.722247	296075.700486	37.859776
1937.492148	296588.440116	37.864794
1939.494223	297116.098785	37.869812
1941.479513	297634.664914	37.874829
1943.389227	298159.920737	37.879847
1945.263988	298690.538697	37.884864
1947.332739	299220.131329	37.889882
1949.152834	299743.057147	37.894900
1951.072666	300271.906846	37.899917
1952.729052	300809.102256	37.904935
1954.973973	301344.648246	37.909952
1956.933460	301880.466939	37.914970
1958.747314	302419.100339	37.919988
1961.308746	302961.238979	37.925005
1962.672992	303493.743451	37.930023
1964.743361	304043.194910	37.935040
1967.103527	304580.404730	37.940058
1968.583552	305124.537507	37.945076
1971.315281	305674.758538	37.950093
1973.123896	306218.398492	37.955111
1975.016844	306759.532255	37.960128
1976.932584	307300.912758	37.965146
1978.491738	307852.176795	37.970164
1980.936623	308383.837899	37.975181
1982.748337	308939.725746	37.980199
1984.869554	309495.558676	37.985216
1987.102415	310039.966934	37.990234
1989.101252	310588.092354	37.995252
1991.330197	311122.437411	38.000269
1993.005526	311670.278516	38.005287
1995.205687	312217.546568	38.010304
1997.350131	312760.350509	38.015322
1999.325597	313308.485780	38.020340
2001.304217	313844.782990	38.025357
2003.779017	314399.760261	38.030375
2005.097686	314941.364119	38.035392
2007.069461	315470.083297	38.040410
2009.197151	316024.191271	38.045428
2011.266043	316558.396641	38.050445
2013.324233	317083.763079	38.055463
2015.317269	317604.260962	38.060480
2017.690497	318120.527822	38.065498
2019.037066	318638.483823	38.070516
2021.541854	319146.164067	38.075533
2023.539297	319670.657378	38.080551
2025.549789	320193.747882	38.085568
2027.502648	320708.312294	38.090586
2029.067463	321237.917487	38.095604
2031.101853	321759.391933	38.100621
2032.930689	322298.288719	38.105639
2034.785478	322839.715731	38.110656
2037.149735	323381.460255	38.115674
2038.746216	323921.143334	38.120692
2040.835020	324461.781449	38.125709
2042.866152	325014.128958	38.130727
2044.484224	325570.449654	38.135744
2046.884410	326128.565714	38.140762
2048.530699	326693.148300	38.145780
2050.627702	327248.638187	38.150797
2052.780458	327819.245157	38.155815
2054.613766	328409.219714	38.160832
2056.918995	328983.192198	38.165850
2058.801135	329571.039715	38.170868
2061.010128	330142.782439	38.175885
2063.014346	330720.950787	38.180903
2064.816623	331310.443710	38.185920
2067.446593	331890.400754	38.190938
2069.039073	332483.622372	38.195956
2071.631674	333074.540074	38.200973
2073.693398	333661.578860	38.205991
2075.636569	334256.068822	38.211008
2077.963338	334852.849721	38.216026
2079.589191	335446.896561	38.221044
2081.909164	336045.518316	38.226061
2084.299720	336638.029366	38.231079
2086.471788	337242.525655	38.236096
2088.824563	337834.826241	38.241114
2090.766126	338436.529009	38.246132
2092.923129	339031.386431	38.251149
2095.130827	339624.020191	38.256167
2097.068271	340233.317166	38.261184
2099.658871	340825.721208	38.266202
2101.156463	341436.776668	38.271220
2103.540568	342035.291954	38.276237
2105.744710	342626.875132	38.281255
2107.756527	343238.076985	38.286272
2110.215813	343836.405343	38.291290
2112.112722	344446.722445	38.296308
2114.422514	345033.182439	38.301325
2116.449192	345644.680906	38.306343
2118.586433	346248.057108	38.311360
2121.178610	346851.121966	38.316378
2122.849561	347451.006409	38.321396
2124.839424	348055.804526	38.326413
2127.498786	348657.083432	38.331431
2129.296011	349267.048957	38.336448
2132.061594	349861.061620	38.341466
2133.865868	350469.486964	38.346484
2136.142121	351065.239210	38.351501
2138.733045	351667.630811	38.356519
2140.184352	352266.725732	38.361536
2142.821667	352862.596920	38.366554
2144.601151	353473.750546	38.371572
2146.826255	354070.129829	38.376589
2149.016543	354662.446589	38.381607
2151.249871	355270.708355	38.386624
2153.411229	355867.301248	38.391642
2155.109179	356438.867744	38.396660
2157.453656	357010.877880	38.401677
2159.323523	357579.507752	38.406695
2161.022963	358157.012884	38.411712
2163.624662	358734.335556	38.416730
2165.275191	359317.363449	38.421748
2167.268450	359911.921072	38.426765
2169.461995	360499.079255	38.431783
2171.389687	361095.076294	38.436800
2173.611558	361686.601415	38.441818
2175.757852	362302.282235	38.446836
2177.637149	362903.714481	38.451853
2179.835555	363521.574664	38.456871
2181.853086	364141.661936	38.461888
2184.303075	364749.465740	38.466906
2186.218952	365378.479467	38.471924
2188.357526	366016.426113	38.476941
2190.562088	366636.619620	38.481959
2192.706264	367270.789852	38.486976
2194.946117	367904.121840	38.491994
2196.947594	368542.175054	38.497012
2199.174275	369195.652890	38.502029
2201.524757	369836.314839	38.507047
2203.400520	370489.320265	38.512064
2206.013430	371136.764425	38.517082
2208.177023	371804.764796	38.522100
2210.140345	372459.318089	38.527117
2212.842510	373117.186740	38.532135
2214.624788	373774.053753	38.537152
2216.949669	374441.470837	38.542170
2219.214415	375109.062692	38.547188
2221.512178	375781.480200	38.552205
2223.806827	376448.737106	38.557223
2225.816942	377132.156765	38.562240
2228.316147	377799.379084	38.567258
2230.655481	378479.446179	38.572276
2232.872306	379155.259711	38.577293
2235.118147	379825.881978	38.582311
2237.593985	380513.492808	38.587328
2240.074134	381184.860585	38.592346
2242.220075	381864.612060	38.597364
2244.493846	382541.894308	38.602381
2246.824606	383219.863107	38.607399
2248.644994	383906.116889	38.612416
2251.195194	384587.570591	38.617434
2253.563047	385279.840523	38.622452
2255.796083	385961.342837	38.627469
2257.931672	386644.317117	38.632487
2260.210604	387337.875411	38.637504
2262.619697	388022.955059	38.642522
2264.596578	388717.546869	38.647540
2267.250270	389399.564670	38.652557
2269.711918	390094.780919	38.657575
2271.848581	390777.360720	38.662592
2274.447989	391470.292510	38.667610
2276.928079	392164.444984	38.672628
2279.061931	392849.843295	38.677645
2281.741766	393525.580305	38.682663
2283.936169	394216.209698	38.687680
2285.902414	394895.151231	38.692698
2288.175925	395581.401949	38.697716
2290.301205	396267.534532	38.702733
2292.815059	396949.379979	38.707751
2295.149804	397641.351050	38.712768
2297.691167	398321.918190	38.717786
2299.864997	399011.779850	38.722804
2302.332749	399689.032606	38.727821
2304.605822	400355.024937	38.732839
2306.598146	401022.340467	38.737856
2308.951556	401675.238609	38.742874
2311.117684	402330.635857	38.747892
2313.281957	402980.165042	38.752909
2315.435845	403638.447815	38.757927
2317.442586	404308.267811	38.762944
2319.858909	404957.430812	38.767962
2322.213768	405634.686365	38.772980
2324.327441	406296.459872	38.777997
2326.789087	406965.608434	38.783015
2328.984997	407645.146136	38.788032
2331.525861	408329.372647	38.793050
2333.972055	409014.610822	38.798068
2335.862200	409706.079079	38.803085
2338.734077	410382.396584	38.808103
2340.845905	411070.981236	38.813120
2343.342102	411754.393264	38.818138
2345.228190	412446.880345	38.823156
2347.428304	413161.840141	38.828173
2349.727128	413859.540996	38.833191
2352.006111	414568.193316	38.838208
2354.520956	415277.293941	38.843226
2357.095414	415999.433588	38.848244
2359.438514	416709.004443	38.853261
2361.875739	417423.807680	38.858279
2364.132183	418141.203788	38.863296
2366.932107	418868.948478	38.868314
2369.088420	419582.471200	38.873332
2371.816183	420306.615868	38.878349
2373.872703	421034.749838	38.883367
2376.481849	421754.643538	38.888384
2378.845585	422486.938172	38.893402
2381.280971	423210.565568	38.898420
2383.690789	423949.214882	38.903437
2386.401783	424673.968962	38.908455
2388.903500	425405.065201	38.913472
2390.828750	426127.171494	38.918490
2393.581051	426859.296422	38.923508
2395.975406	427603.912794	38.928525
2398.376492	428336.455695	38.933543
2400.804133	429075.755548	38.938560
2403.113036	429810.394595	38.943578
2405.668025	430556.562737	38.948596
2407.832848	431302.822245	38.953613
2410.623009	432041.058242	38.958631
2413.066295	432788.388667	38.963648
2415.480503	433528.866725	38.968666
2418.023882	434263.529759	38.973684
2420.547388	435013.002155	38.978701
2423.084720	435744.025400	38.983719
2425.369712	436483.923538	38.988736
2427.860974	437236.820370	38.993754
2430.531837	437963.347419	38.998772
2432.504298	438715.217908	39.003789
2435.217052	439459.502498	39.008807
2437.451996	440198.831671	39.013824
2440.128497	440943.325787	39.018842
2442.634606	441689.037381	39.023860
2445.018343	442447.038805	39.028877
2447.579730	443178.574655	39.033895
2449.800179	443945.202918	39.038912
2452.317282	444681.653854	39.043930
2454.790301	445427.344897	39.048948
2456.912252	446177.317506	39.053965
2459.715397	446909.547888	39.058983
2462.130323	447666.249301	39.064000
2464.165935	448417.877753	39.069018
2467.137484	449160.018511	39.074036
2469.336365	449899.124930	39.079053
2471.899735	450611.036272	39.084071
2474.140596	451336.682565	39.089088
2476.508629	452061.220730	39.094106
2479.238557	452775.155194	39.099124
2481.311687	453502.726215	39.104141
2483.953810	454229.065332	39.109159
2485.927691	454958.826525	39.114176
2488.257067	455690.930274	39.119194
2490.793453	456428.080535	39.124212
2493.467439	457172.967825	39.129229
2495.687586	457916.790421	39.134247
2498.024165	458674.671891	39.139264
2500.295789	459441.332195	39.144282
2503.016921	460193.279264	39.149300
2505.187907	460968.441306	39.154317
2508.154081	461735.455267	39.159335
2510.403500	462514.487023	39.164352
2512.599409	463291.424602	39.169370
2515.226871	464076.044028	39.174388
2517.550811	464864.776026	39.179405
2520.089580	465649.195500	39.184423
2522.736756	466449.838461	39.189440
2525.224791	467254.921734	39.194458
2528.194588	468046.905055	39.199476
2529.992026	468872.399537	39.204493
2533.094545	469680.463477	39.209511
2535.719705	470498.172020	39.214528
2537.881027	471312.941026	39.219546
2540.630176	472122.222699	39.224564
2543.290752	472948.206393	39.229581
2545.726618	473763.279070	39.234599
2548.264428	474591.433499	39.239616
2551.032302	475417.694749	39.244634
2554.064052	476233.773542	39.249652
2556.366480	477066.352033	39.254669
2559.132992	477883.916978	39.259687
2562.061085	478719.802422	39.264704
2564.222949	479547.544291	39.269722
2566.787193	480369.071754	39.274740
2569.309952	481207.687493	39.279757
2572.203676	482037.669518	39.284775
2574.850848	482884.922469	39.289792
2577.564504	483706.525920	39.294810
2580.225155	484538.702843	39.299828
2582.611481	485373.662863	39.304845
2585.169466	486197.600443	39.309863
2588.372555	487030.479765	39.314880
2590.776462	487870.619486	39.319898
2593.491309	488698.200127	39.324916
2596.097564	489538.428396	39.329933
2598.534953	490371.477093	39.334951
2601.351848	491202.000706	39.339968
2603.561467	492036.167720	39.344986
2606.301818	492877.675456	39.350004
2608.719160	493717.731844	39.355021
2611.688859	494560.431094	39.360039
2614.431466	495396.667705	39.365056
2616.867348	496246.939911	39.370074
2619.537071	497074.831294	39.375092
2622.230465	497923.816195	39.380109
2624.666407	498761.904236	39.385127
2627.493276	499607.805492	39.390144
2630.138585	500444.816115	39.395162
2632.788611	501283.347386	39.400180
2635.286070	502124.786641	39.405197
2637.987718	502961.912869	39.410215
2640.665906	503795.772741	39.415232
2643.034626	504602.208106	39.420250
2646.040963	505403.506270	39.425268
2648.474172	506216.910724	39.430285
2650.495591	507017.535356	39.435303
2652.998807	507828.074134	39.440320
2655.753179	508648.260963	39.445338
2658.078014	509465.199856	39.450356
2660.484331	510297.811743	39.455373
2663.252216	511135.361306	39.460391
2666.140841	511959.438942	39.465408
2668.443371	512806.402822	39.470426
2670.765816	513646.110742	39.475444
2673.551418	514495.071332	39.480461
2675.951152	515362.242017	39.485479
2678.482744	516218.055035	39.490496
2680.775227	517098.248692	39.495514
2683.602093	517966.060420	39.500532
2686.015670	518860.040477	39.505549
2688.952665	519747.584759	39.510567
2691.656428	520630.179177	39.515584
2694.019063	521540.132224	39.520602
2696.545332	522436.806626	39.525620
2699.526319	523338.138058	39.530637
2701.530298	524268.889570	39.535655
2704.615115	525183.793044	39.540672
2707.218517	526119.719941	39.545690
2710.526636	527040.365262	39.550708
2713.694437	527974.471433	39.555725
2716.076675	528897.823244	39.560743
2719.155370	529824.778581	39.565760
2721.647727	530755.095027	39.570778
2724.561294	531687.598762	39.575796
2727.625940	532616.192585	39.580813
2730.387577	533555.649379	39.585831
2733.536276	534478.221575	39.590848
2736.020842	535416.546679	39.595866
2739.074759	536349.634177	39.600884
2741.916451	537278.267932	39.605901
2744.359508	538222.002530	39.610919
2747.184450	539150.567880	39.615936
2749.797683	540099.332548	39.620954
2752.687349	541033.801473	39.625972
2755.561761	541972.990043	39.630989
2758.244971	542922.861605	39.636007
2760.913054	543859.895868	39.641024
2763.586426	544820.303503	39.646042
2766.696746	545765.234318	39.651060
2769.474418	546716.843910	39.656077
2772.203878	547669.904562	39.661095
2775.183895	548626.528514	39.666112
2778.085998	549591.494955	39.671130
2780.831521	550533.142827	39.676148
2783.688187	551489.285634	39.681165
2786.556261	552441.539165	39.686183
2789.186532	553389.543005	39.691200
2791.833664	554350.042336	39.696218
2794.930931	555304.720091	39.701236
2797.561690	556257.597827	39.706253
2800.539770	557221.756781	39.711271
2803.591519	558180.005501	39.716288
2806.167170	559119.473504	39.721306
2808.891042	560073.570014	39.726324
2812.044104	561027.376096	39.731341
2814.558728	561987.045020	39.736359
2817.476090	562946.275952	39.741376
2820.081545	563891.626441	39.746394
2822.613312	564851.684918	39.751412
2825.797505	565795.646540	39.756429
2828.415848	566729.188572	39.761447
2831.193317	567653.247884	39.766464
2833.876893	568575.248104	39.771482
2836.633653	569493.053468	39.776500
2839.164787	570420.166850	39.781517
2842.304776	571344.401904	39.786535
2845.311622	572271.050966	39.791552
2848.105918	573204.392229	39.796570
2850.576605	574133.853776	39.801588
2853.627972	575074.792423	39.806605
2855.951949	576007.953106	39.811623
2859.221996	576964.217831	39.816640
2862.093856	577917.615298	39.821658
2864.810492	578871.466839	39.826676
2867.022158	579838.620525	39.831693
2869.624403	580801.872370	39.836711
2872.409633	581785.931960	39.841728
2875.374516	582778.006920	39.846746
2877.884334	583755.935912	39.851764
2881.195878	584755.314561	39.856781
2883.800116	585750.716788	39.861799
2886.873658	586757.088965	39.866816
2889.889829	587766.093553	39.871834
2892.783760	588775.534901	39.876852
2895.625259	589790.012025	39.881869
2898.433265	590813.128470	39.886887
2901.660690	591834.083491	39.891904
2904.532343	592867.936663	39.896922
2906.945251	593891.303998	39.901940
2910.341206	594921.183564	39.906957
2913.187768	595968.996634	39.911975
2915.829345	597001.673326	39.916992
2918.985857	598048.898407	39.922010
2921.670713	599101.415444	39.927028
2925.018556	600140.958702	39.932045
2927.666579	601209.214020	39.937063
2930.829661	602250.650673	39.942080
2933.590305	603319.092122	39.947098
2936.778118	604377.502420	39.952116
2939.910822	605436.073924	39.957133
2942.785408	606502.496890	39.962151
2945.692203	607561.458087	39.967168
2948.989191	608628.962246	39.972186
2952.236544	609698.724971	39.977204
2954.807875	610745.534461	39.982221
2957.722467	611838.560920	39.987239
2960.853899	612900.633345	39.992256
2963.571289	613975.676106	39.997274
2966.408867	615054.645496	40.002292
2970.009123	616119.282735	40.007309
2972.694487	617212.617217	40.012327
2975.943058	618279.153241	40.017344
2978.807967	619370.393097	40.022362
2981.769076	620445.413096	40.027380
2984.978068	621518.336749	40.032397
2987.983272	622602.931678	40.037415
2991.074135	623676.410406	40.042432
2994.040411	624761.244426	40.047450
2996.985277	625842.725009	40.052468
2999.407877	626915.190686	40.057485
3002.590670	628008.651486	40.062503
3005.331917	629101.373414	40.067520
3008.202266	630194.960176	40.072538
3011.344937	631302.270307	40.077556
3014.371639	632385.767282	40.082573
3017.215745	633482.062653	40.087591
3020.370390	634582.285230	40.092608
3023.032019	635673.089509	40.097626
3026.013797	636738.972593	40.102644
3029.140917	637806.818014	40.107661
3031.661083	638873.755020	40.112679
3034.794347	639937.536861	40.117696
3037.887519	641007.750299	40.122714
3040.686887	642079.047607	40.127732
3043.473618	643153.825684	40.132749
3046.149985	644244.816254	40.137767
3049.305048	645329.876096	40.142784
3052.196176	646431.665920	40.147802
3054.779323	647539.069583	40.152820
3057.622616	648645.610517	40.157837
3060.717828	649765.395677	40.162855
3063.842389	650897.210949	40.167872
3066.398171	652026.948262	40.172890
3069.376602	653170.438793	40.177908
3072.570083	654320.188638	40.182925
3075.670778	655491.040894	40.187943
3078.715824	656646.870097	40.192960
3081.611026	657819.072510	40.197978
3084.779366	658988.201074	40.202996
3087.805279	660168.963454	40.208013
3090.774902	661358.254087	40.213031
3093.714721	662544.864786	40.218048
3097.226841	663735.266767	40.223066
3100.039400	664942.806072	40.228084
3103.417596	666133.380642	40.233101
3106.321301	667355.329451	40.238119
3109.264971	668557.464674	40.243136
3112.574803	669779.333458	40.248154
3115.524815	671012.393492	40.253172
3119.084871	672231.516523	40.258189
3122.268172	673467.001360	40.263207
3125.039160	674693.691109	40.268224
3128.481239	675920.954146	40.273242
3131.309998	677171.516320	40.278260
3134.998284	678401.840497	40.283277
3137.904667	679657.918173	40.288295
3141.398476	680900.313790	40.293312
3144.374342	682145.309197	40.298330
3147.446098	683396.973740	40.303348
3151.180127	684638.673492	40.308365
3153.999557	685894.406747	40.313383
3157.237349	687153.372491	40.318400
3160.547817	688395.024822	40.323418
3163.640209	689656.345895	40.328436
3167.120085	690900.751289	40.333453
3170.376069	692175.586478	40.338471
3173.756661	693417.524077	40.343488
3177.068214	694661.432673	40.348506
3180.119996	695923.759572	40.353524
3183.277450	697173.094027	40.358541
3186.393762	698432.522136	40.363559
3189.522303	699682.645283	40.368576
3192.816232	700937.618828	40.373594
3195.658383	702211.766506	40.378612
3199.353687	703467.399790	40.383629
3202.308896	704732.783889	40.388647
3205.828908	705981.392211	40.393664
3209.092967	707251.359743	40.398682
3211.717264	708519.164775	40.403700
3215.151774	709766.295849	40.408717
3218.487339	711049.949813	40.413735
3221.566870	712321.868089	40.418752
3224.890782	713586.675139	40.423770
3228.174658	714854.367940	40.428788
3231.335731	716119.564585	40.433805
3234.426808	717371.867046	40.438823
3237.545274	718598.402726	40.443840
3240.649491	719817.687668	40.448858
3243.949000	721038.888352	40.453876
3247.313462	722261.035910	40.458893
3250.556587	723482.676888	40.463911
3253.504086	724704.976611	40.468928
3256.794285	725930.695649	40.473946
3260.076037	727153.070208	40.478964
3263.076065	728374.863785	40.483981
3266.671601	729628.042893	40.488999
3269.444058	730868.173706	40.494016
3272.901948	732106.618980	40.499034
3276.383103	733364.622313	40.504052
3279.575773	734621.193080	40.509069
3282.451234	735870.363068	40.514087
3285.847412	737136.773801	40.519104
3289.067771	738384.951179	40.524122
3292.159474	739681.406307	40.529140
3295.528257	740956.193799	40.534157
3298.866645	742242.668060	40.539175
3302.055787	743534.085988	40.544192
3305.882364	744822.573466	40.549210
3308.712841	746132.360188	40.554228
3312.169093	747428.909917	40.559245
3315.516004	748737.632066	40.564263
3318.647446	750053.314134	40.569280
3322.642937	751370.453175	40.574298
3325.342483	752684.871859	40.579316
3328.850350	753987.556202	40.584333
3332.398724	755313.648618	40.589351
3335.828517	756637.906031	40.594368
3339.310612	757965.419822	40.599386
3342.705590	759290.944439	40.604404
3346.079998	760631.494835	40.609421
3349.468032	761962.605126	40.614439
3352.817686	763288.518421	40.619456
3356.397545	764627.487743	40.624474
3359.357536	765976.252530	40.629492
3362.969043	767316.062760	40.634509
3366.480011	768660.858705	40.639527
3370.008816	770011.010534	40.644544
3373.616105	771352.451546	40.649562
3377.143138	772702.652074	40.654580
3380.458667	774037.412803	40.659597
3384.101356	775381.993113	40.664615
3387.424129	776722.008807	40.669632
3391.580294	778065.568025	40.674650
3394.655211	779419.609532	40.679668
3398.066705	780757.835359	40.684685
3401.613041	782100.648265	40.689703
3405.012108	783454.076039	40.694720
3408.970040	784789.745348	40.699738
3412.303753	786130.122766	40.704756
3415.899589	787467.900893	40.709773
3419.500593	788804.838346	40.714791
3422.512268	790144.022294	40.719808
3426.532801	791481.071427	40.724826
3429.537098	792821.267756	40.729844
3433.099636	794154.847082	40.734861
3436.722045	795499.817980	40.739879
3440.203549	796849.302531	40.744896
3443.703891	798195.144893	40.749914
3447.132106	799536.725091	40.754932
3450.867480	800885.090185	40.759949
3454.637807	802221.053135	40.764967
3457.807346	803547.121901	40.769984
3461.618955	804881.436074	40.775002
3465.048601	806205.202161	40.780007
3468.323599	807459.081376	40.785012
3471.968809	808676.749736	40.790016
3475.304486	809829.480376	40.795021
3478.361321	810912.549141	40.800026
3481.431713	811930.104116	40.805031
3484.517183	812885.063669	40.810036
3487.251213	813766.301328	40.815040
3489.904532	814571.940777	40.820045
3492.745001	815315.916984	40.825050
3494.995277	816001.902779	40.830055
3497.253648	816608.379429	40.835060
3500.126417	817149.755197	40.840064
3501.692845	817650.831073	40.845069
3504.198621	818074.056171	40.850074
3505.739063	818445.007849	40.855079
3507.330279	818756.041265	40.860084
3509.040445	819017.232634	40.865088
3510.382974	819242.807542	40.870093
3511.979046	819409.330341	40.875098
3513.689790	819545.888961	40.880103
3514.771688	819626.336221	40.885108
3515.861566	819673.465029	40.890112
3517.209294	819688.017687	40.895117
3518.455547	819654.740839	40.900122
3519.162147	819588.970003	40.905127
3520.186106	819495.210778	40.910132
3520.881626	819381.543109	40.915136
3521.748658	819228.557939	40.920141
3522.269197	819044.459816	40.925146
3523.061257	818868.825417	40.930151
3523.966355	818642.818869	40.935156
3524.166484	818407.036575	40.940160
3524.376087	818151.670909	40.945165
3525.170573	817870.752529	40.950170
3525.537105	817607.314672	40.955175
3525.745306	817296.567684	40.960180
3526.449991	816970.699126	40.965184
3526.440721	816652.910293	40.970189
3526.780993	816313.267280	40.975194
3526.412282	815969.269400	40.980199
3526.791838	815599.185802	40.985204
3527.266584	815244.976467	40.990208
3527.246269	814878.247861	40.995213
3527.398823	814487.137363	41.000218
3527.392509	814101.807925	41.005223
3527.386039	813717.043997	41.010228
3527.485712	813325.678710	41.015232
3527.361321	812922.231509	41.020237
3527.707363	812528.428618	41.025242
3527.314640	812111.362043	41.030247
3527.385946	811709.720136	41.035252
3527.512700	811293.986868	41.040256
3527.375776	810887.970840	41.045261
3527.523355	810474.339146	41.050266
3527.740754	810065.031022	41.055271
3527.722503	809638.000553	41.060276
3527.773999	809221.613438	41.065280
3527.389773	808792.336084	41.070285
3527.609318	808349.063698	41.075290
3527.224872	807927.964618	41.080295
3527.101317	807509.541112	41.085300
3527.156988	807075.720936	41.090304
3526.927231	806659.419353	41.095309
3526.860193	806227.575156	41.100314
3526.882479	805797.944015	41.105319
3526.489540	805379.924528	41.110324
3526.525925	804946.903812	41.115328
3526.459656	804533.828871	41.120333
3526.168343	804101.348069	41.125338
3525.909931	803689.921164	41.130343
3525.742872	803272.079169	41.135348
3525.763277	802847.265617	41.140352
3525.701218	802445.786005	41.145357
3525.658656	802031.428606	41.150362
3525.508569	801623.489987	41.155367
3525.369930	801212.581991	41.160372
3525.488419	800783.896837	41.165376
3524.809563	800391.033668	41.170381
3525.010883	799970.477779	41.175386
3524.845655	799560.653541	41.180391
3524.655613	799162.291698	41.185396
3524.556724	798763.695660	41.190400
3524.272982	798372.370480	41.195405
3524.147105	797960.433109	41.200410
3524.189795	797555.118719	41.205415
3523.783838	797150.001903	41.210420
3524.008772	796761.300119	41.215424
3523.541134	796369.598087	41.220429
3523.731653	795975.212780	41.225434
3523.396535	795591.496521	41.230439
3523.137637	795197.828726	41.235444
3523.072149	794806.463775	41.240448
3522.809161	794430.429949	41.245453
3522.678479	794046.693508	41.250458
3522.398757	793675.434392	41.255463
3522.119824	793290.895293	41.260468
3522.316784	792927.916257	41.265472
3521.710821	792558.616444	41.270477
3522.117883	792209.564078	41.275482
3521.942878	791828.955723	41.280487
3521.682673	791462.439657	41.285492
3521.364765	791101.023285	41.290496
3521.325019	790743.522084	41.295501
3521.133874	790382.146293	41.300506
3520.947753	790035.049398	41.305511
3520.676891	789683.379690	41.310516
3520.731654	789340.483972	41.315520
3520.428230	788990.455971	41.320525
3520.558466	788632.525293	41.325530
3520.059935	788307.608470	41.330535
3519.913671	787955.341071	41.335540
3520.170812	787622.060497	41.340544
3520.169923	787299.129088	41.345549
3519.498682	786948.077991	41.350554
3519.227993	786628.503229	41.355559
3519.266349	786300.997552	41.360564
3519.086592	785973.021153	41.365568
3518.920525	785661.546845	41.370573
3518.742248	785332.311659	41.375578
3518.634281	785022.324102	41.380583
3518.349764	784703.452178	41.385588
3518.388082	784395.281878	41.390592
3518.044983	784082.194423	41.395597
3518.141159	783767.053803	41.400602
3517.953144	783473.486991	41.405607
3517.617194	783172.112623	41.410612
3518.038307	782855.009525	41.415616
3517.367749	782561.435764	41.420621
3517.783360	782260.833901	41.425626
3517.388124	781968.272715	41.430631
3516.975469	781669.110759	41.435636
3517.041974	781377.039794	41.440640
3516.951564	781090.443636	41.445645
3516.334253	780799.839468	41.450650
3516.221313	780530.394922	41.455655
3516.386435	780259.762874	41.460660
3516.363340	779979.310973	41.465664
3515.692819	779709.878518	41.470669
3516.013459	779442.093396	41.475674
3516.031911	779171.543246	41.480679
3515.589381	778902.633707	41.485684
3515.697324	778632.393174	41.490688
3515.118959	778378.840998	41.495693
3515.395517	778109.242216	41.500698
3515.260781	777854.860407	41.505703
3515.075805	777594.276269	41.510708
3515.170793	777340.724585	41.515712
3514.909346	777098.002701	41.520717
3515.017044	776837.933942	41.525722
3514.974689	776578.175989	41.530727
3514.634888	776331.995623	41.535732
3514.501345	776082.671466	41.540736
3514.172214	775838.294197	41.545741
3514.440017	775588.493185	41.550746
3514.147850	775349.853796	41.555751
3513.775540	775111.121348	41.560756
3513.955785	774866.578424	41.565760
3513.543591	774652.998329	41.570765
3513.711096	774410.116411	41.575770
3513.450528	774187.634309	41.580775
3513.194905	773961.254333	41.585780
3513.042554	773730.959925	41.590784
3512.953224	773520.494614	41.595789
3513.256539	773292.672239	41.600794
3513.162078	773065.154595	41.605799
3512.960873	772851.388769	41.610804
3513.083031	772626.579962	41.615808
3512.541599	772405.961775	41.620813
3512.734505	772199.401775	41.625818
3513.004440	771988.833427	41.630823
3512.585927	771777.978424	41.635828
3512.638526	771559.256613	41.640832
3512.060196	771356.001979	41.645837
3512.275665	771143.349464	41.650842
3512.182077	770944.240255	41.655847
3512.019167	770736.811157	41.660852
3511.980418	770532.361084	41.665856
3511.580896	770344.026374	41.670861
3511.377114	770142.992255	41.675866
3511.375998	769948.817253	41.680871
3511.394411	769757.393200	41.685876
3511.325763	769564.598878	41.690880
3511.375749	769399.817443	41.695885
3511.238844	769177.163658	41.700890
3511.014877	768994.629572	41.705895
3510.946777	768814.726365	41.710900
3510.969776	768627.461071	41.715904
3510.870389	768446.617777	41.720909
3510.705295	768250.996171	41.725914
3510.855604	768081.536378	41.730919
3510.489457	767912.552095	41.735924
3510.680602	767736.424266	41.740928
3510.371758	767562.937577	41.745933
3510.277794	767378.124430	41.750938
3509.919326	767214.495442	41.755943
3509.874677	767050.022503	41.760948
3510.236348	766879.465416	41.765952
3510.159489	766704.343168	41.770957
3509.932280	766543.388914	41.775962
3509.940036	766371.054643	41.780967
3509.766395	766209.295634	41.785972
3509.759633	766045.237958	41.790976
3509.749836	765891.332594	41.795981
3509.656899	765713.133252	41.800986
3509.593670	765555.581628	41.805991
3509.175267	765413.516515	41.810996
3509.653310	765245.318694	41.816000
3509.472128	765096.947078	41.821005
3509.469061	764940.358650	41.826010
3509.412434	764784.564658	41.831015
3508.919394	764621.985736	41.836020
3509.295687	764479.574724	41.841024
3509.313617	764320.898976	41.846029
3509.122054	764172.905231	41.851034
3509.199841	764025.455909	41.856039
3508.789060	763880.993559	41.861044
3509.271340	763732.830794	41.866048
3508.774415	763588.229064	41.871053
3508.895468	763429.122961	41.876058
3508.694866	763285.354231	41.881063
3508.609497	763150.243408	41.886068
3508.799216	763017.106830	41.891072
3508.371428	762882.738057	41.896077
3508.361270	762725.463443	41.901082
3508.304375	762584.123570	41.906087
3507.911222	762457.386064	41.911092
3508.655632	762328.535450	41.916096
3508.626620	762194.927154	41.921101
3508.288503	762061.564712	41.926106
3508.273861	761918.922990	41.931111
3508.244686	761791.769041	41.936116
3508.254424	761654.001467	41.941120
3507.997955	761535.759316	41.946125
3507.940840	761394.101200	41.951130
3507.724791	761266.229269	41.956135
3507.831452	761138.400657	41.961140
3507.900157	761017.778334	41.966144
3507.903757	760892.577039	41.971149
3507.872191	760772.312636	41.976154
3507.906603	760642.563605	41.981159
3507.645713	760522.530343	41.986164
3508.021285	760385.123347	41.991168
3507.851099	760271.385932	41.996173
3507.803229	760134.340163	42.001178
3507.700729	760008.204329	42.006183
3507.726871	759890.333893	42.011188
3507.544530	759769.535681	42.016192
3507.325652	759654.119513	42.021197
3507.455654	759525.223681	42.026202
3507.255532	759413.402563	42.031207
3507.118810	759290.122163	42.036212
3507.410144	759166.670544	42.041216
3507.243701	759064.904531	42.046221
3507.303787	758942.967660	42.051226
3507.019907	758833.273564	42.056231
3507.010887	758723.927354	42.061236
3507.113977	758609.675868	42.066240
3507.010589	758490.768763	42.071245
3507.171927	758372.210957	42.076250
3507.010220	758266.535024	42.081255
3506.890718	758175.309820	42.086260
3506.903809	758049.122366	42.091264
3506.892750	757955.606586	42.096269
3507.183672	757835.390510	42.101274
3506.796784	757723.673984	42.106279
3506.750209	757622.559823	42.111284
3506.841119	757519.250140	42.116288
3506.690678	757413.165673	42.121293
3506.696354	757292.988035	42.126298
3506.592121	757193.654435	42.131303
3506.238252	757090.708357	42.136308
3506.605054	756990.751589	42.141312
3506.451983	756890.286887	42.146317
3506.478139	756787.422167	42.151322
3506.260395	756687.607100	42.156327
3506.569596	756599.796820	42.161332
3506.430384	756494.339380	42.166336
3506.361582	756401.751874	42.171341
3506.295361	756297.414967	42.176346
3506.483305	756196.687502	42.181351
3505.884818	756102.455992	42.186356
3506.344264	756004.544256	42.191360
3505.971185	755923.848120	42.196365
3505.849615	755829.880207	42.201370
3505.869419	755735.986574	42.206375
3506.212263	755645.543475	42.211380
3506.077472	755552.660363	42.216384
3505.808128	755458.514773	42.221389
3505.749719	755359.001653	42.226394
3506.118053	755276.646150	42.231399
3505.992026	755186.817929	42.236404
3506.098153	755082.337308	42.241408
3506.092041	754998.312610	42.246413
3505.893372	754918.268291	42.251418
3506.225915	754821.547211	42.256423
3505.870480	754736.984760	42.261428
3506.006192	754638.960796	42.266432
3505.753278	754550.627164	42.271437
3505.629746	754460.938135	42.276442
3505.918547	754370.390146	42.281447
3505.528923	754287.655178	42.286452
3505.665807	754193.081482	42.291456
3505.507207	754116.675890	42.296461
3505.392643	754026.140928	42.301466
3505.340988	753955.591781	42.306471
3505.468839	753869.804490	42.311476
3505.685046	753790.272554	42.316480
3505.371331	753709.790184	42.321485
3505.496371	753634.468738	42.326490
3505.284857	753547.104289	42.331495
3505.067029	753469.961342	42.336500
3505.485568	753389.601860	42.341504
3505.419958	753312.432252	42.346509
3505.324850	753225.736289	42.351514
3505.666347	753159.213637	42.356519
3505.342560	753072.109193	42.361524
3505.221232	752979.735900	42.366528
3505.245392	752913.214027	42.371533
3505.309808	752821.302053	42.376538
3505.407373	752746.124587	42.381543
3504.964812	752673.702125	42.386548
3505.340158	752595.415604	42.391552
3505.255972	752517.648471	42.396557
3504.999094	752449.045336	42.401562
3505.120141	752377.811248	42.406567
3504.924446	752306.332373	42.411572
3504.980060	752224.489557	42.416576
3504.882276	752148.054382	42.421581
3504.912715	752087.697777	42.426586
3505.088489	752011.611279	42.431591
3504.744187	751940.894326	42.436596
3504.976617	751857.684987	42.441600
3504.741468	751784.577927	42.446605
3504.583631	751726.620228	42.451610
3504.691374	751650.393208	42.456615
3504.453851	751604.400247	42.461620
3504.667025	751532.402311	42.466624
3504.541086	751484.908510	42.471629
3504.670330	751412.034230	42.476634
3505.067511	751344.103770	42.481639
3504.506374	751266.797752	42.486644
3504.730228	751197.560949	42.491648
3504.729881	751123.421069	42.496653
3504.470636	751065.919665	42.501658
3504.692151	750990.754068	42.506663
3504.460255	750937.544554	42.511668
3504.837419	750863.685747	42.516672
3504.480785	750808.717655	42.521677
3504.440874	750745.200804	42.526682
3504.742270	750670.512899	42.531687
3504.448766	750623.436589	42.536692
3504.578701	750545.268524	42.541696
3504.532069	750487.036214	42.546701
3504.652964	750420.279325	42.551706
3504.730309	750349.280727	42.556711
3504.462814	750279.128688	42.561716
3504.475468	750210.115450	42.566720
3504.609833	750168.350451	42.571725
3504.448759	750094.721197	42.576730
3504.618660	750020.345094	42.581735
3504.390815	749962.632710	42.586740
3504.712927	749911.103304	42.591744
3504.541452	749853.232612	42.596749
3504.518144	749780.565716	42.601754
3504.618107	749717.758430	42.606759
3504.231394	749656.759943	42.611764
3504.492862	749586.712090	42.616768
3504.206127	749534.934679	42.621773
3504.414067	749469.884408	42.626778
3504.523832	749406.924778	42.631783
3504.362210	749353.396366	42.636788
3504.380370	749289.759204	42.641792
3504.188732	749233.369379	42.646797
3504.186550	749171.809656	42.651802
3504.425529	749098.599091	42.656807
3504.590858	749060.874397	42.661812
3504.490162	748988.855131	42.666816
3504.227757	748933.858203	42.671821
3504.326765	748871.192450	42.676826
3504.214816	748808.709177	42.681831
3504.447738	748751.208311	42.686836
3504.607789	748689.469809	42.691840
3504.408847	748636.634338	42.696845
3504.610730	748560.509636	42.701850
3504.636836	748512.923149	42.706855
3504.498627	748445.154339	42.711860
3504.538561	748369.103860	42.716864
3504.603703	748319.533295	42.721869
3504.092570	748257.605485	42.726874
3504.438005	748206.011521	42.731879
3504.252105	748152.034118	42.736884
3503.861083	748090.381662	42.741888
3503.871245	748037.557079	42.746893
3504.085372	747979.460644	42.751898
3504.499105	747911.596244	42.756903
3504.475369	747855.909975	42.761908
3504.596385	747804.646821	42.766912
3504.274350	747742.337843	42.771917
3504.300092	747679.625152	42.776922
3504.504292	747615.993057	42.781927
3504.377606	747560.815805	42.786932
3504.428950	747494.588821	42.791937
3504.398325	747447.054584	42.796941
3504.392007	747388.495894	42.801946
3504.338461	747331.921272	42.806951
3504.020628	747274.351997	42.811956
3504.249939	747204.683350	42.816961
3504.016861	747150.657360	42.821965
3503.946206	747094.528608	42.826970
3504.377957	747035.944511	42.831975
3504.390909	746978.565649	42.836980
3504.281908	746926.642739	42.841985
3504.474412	746857.866634	42.846989
3504.320495	746805.406686	42.851994
3504.418769	746735.360071	42.856999
3503.838135	746690.877165	42.862004
3504.094701	746630.539695	42.867009
3504.150762	746573.496711	42.872013
3503.992699	746529.931719	42.877018
3504.037096	746461.819033	42.882023
3504.217553	746413.255246	42.887028
3504.092883	746355.350818	42.892033
3504.025960	746295.854855	42.897037
3503.985860	746247.326379	42.902042
3504.077871	746192.647092	42.907047
3503.992457	746137.650678	42.912052
3504.346449	746091.379307	42.917057
3504.365373	746036.710974	42.922061
3504.245932	745986.562883	42.927066
3504.224235	745919.296615	42.932071
3504.135474	745869.043861	42.937076
3504.290335	745810.595066	42.942081
3503.747774	745746.971937	42.947085
3504.250722	745704.627991	42.952090
3504.042707	745641.047734	42.957095
3503.934786	745591.735504	42.962100
3503.780723	745535.905875	42.967105
3504.058029	745482.031395	42.972109
3504.034310	745423.707997	42.977114
3504.225848	745370.440044	42.982119
3504.169948	745331.151996	42.987124
3504.309483	745263.260356	42.992129
3503.897450	745219.729911	42.997133
3504.151451	745154.784360	43.002138
3504.242612	745100.740204	43.007143
3503.500281	745044.855707	43.012148
3503.753070	744991.871685	43.017153
3503.950353	744948.189901	43.022157
3503.732128	744907.591778	43.027162
3503.981548	744848.279857	43.032167
3503.698333	744801.957569	43.037172
3503.701355	744757.664088	43.042177
3503.631407	744711.899340	43.047181
3503.651630	744648.075678	43.052186
3503.776248	744609.644101	43.057191
3503.746682	744572.918551	43.062196
3504.226629	744510.550525	43.067201
3504.184691	744458.600187	43.072205
3503.715438	744405.088505	43.077210
3503.771791	744349.561812	43.082215
3503.881105	744305.248265	43.087220
3503.548797	744252.306224	43.092225
3503.836725	744218.591832	43.097229
3503.633940	744156.234614	43.102234
3503.821508	744109.632912	43.107239
3503.318036	744075.306728	43.112244
3503.599575	744013.709033	43.117249
3503.736946	743971.959817	43.122253
3503.904309	743927.881775	43.127258
3503.985355	743882.631150	43.132263
3503.510135	743830.649171	43.137268
3503.544699	743779.719983	43.142273
3503.752787	743728.811314	43.147277
3503.713215	743692.874352	43.152282
3503.828490	743638.222866	43.157287
3503.741114	743590.773448	43.162292
3503.611925	743541.352950	43.167297
3503.654914	743494.969199	43.172301
3503.405387	743451.501045	43.177306
3503.712652	743403.837146	43.182311
3503.548791	743364.161499	43.187316
3503.837936	743309.330751	43.192321
3503.685763	743269.257151	43.197325
3503.369385	743230.397059	43.202330
3504.002957	743177.288625	43.207335
3503.594625	743140.569348	43.212340
3503.830801	743088.910246	43.217345
3503.598569	743035.894074	43.222349
3503.821894	742993.581609	43.227354
3503.840457	742934.886644	43.232359
3503.652761	742899.316587	43.237364
3503.376049	742852.289482	43.242369
3503.685060	742792.507226	43.247373
3503.621288	742748.163985	43.252378
3503.439018	742706.658516	43.257383
3503.669651	742659.151084	43.262388
3503.542015	742622.729272	43.267393
3503.305573	742581.973789	43.272397
3503.365185	742532.614748	43.277402
3503.839024	742495.499862	43.282407
3503.379494	742447.511491	43.287412
3503.649911	742402.765100	43.292417
3503.396183	742363.049767	43.297421
3503.336150	742319.247441	43.302426
3503.521875	742273.475828	43.307431
3503.591239	742241.025244	43.312436
3503.475972	742193.374202	43.317441
3503.507210	742164.143866	43.322445
3503.433991	742103.084200	43.327450
3503.537736	742050.550002	43.332455
3503.621305	742022.052289	43.337460
3503.565519	741962.670018	43.342465
3503.224799	741914.312660	43.347469
3502.830805	741885.596429	43.352474
3503.211193	741848.642263	43.357479
3503.333100	741822.807958	43.362484
3503.406207	741774.233196	43.367489
3503.474823	741733.769238	43.372493
3503.481118	741690.397575	43.377498
3503.270009	741636.082714	43.382503
3502.940520	741611.212266	43.387508
3503.186462	741576.108784	43.392513
3503.381900	741532.606181	43.397517
3503.153835	741501.042293	43.402522
3503.444623	741451.885681	43.407527
3503.270168	741416.504574	43.412532
3503.645949	741373.465935	43.417537
3503.369374	741338.645318	43.422541
3503.328745	741285.041792	43.427546
3503.625014	741250.769331	43.432551
3503.303148	741206.509413	43.437556
3503.389478	741167.622253	43.442561
3503.417677	741131.563539	43.447565
3503.379595	741091.410617	43.452570
3503.488734	741038.868809	43.457575
3503.407023	740997.535614	43.462580
3503.434865	740965.284467	43.467585
3503.536284	740918.232989	43.472589
3503.280956	740878.658827	43.477594
3503.659218	740830.225824	43.482599
3503.253562	740791.417882	43.487604
3503.486503	740749.883170	43.492609
3503.318160	740715.041973	43.497613
3503.469593	740672.234331	43.502618
3503.631301	740625.616321	43.507623
3503.381228	740573.180072	43.512628
3503.306063	740540.548482	43.517633
3503.563728	740504.993176	43.522637
3503.381986	740452.891098	43.527642
3503.598099	740411.703619	43.532647
3503.265183	740366.550511	43.537652
3503.642854	740323.258551	43.542657
3503.641311	740270.532037	43.547661
3503.147165	740228.619773	43.552666
3503.396739	740182.133067	43.557671
3503.375459	740144.940364	43.562676
3503.293256	740106.966108	43.567681
3503.336092	740069.960344	43.572685
3503.305575	740034.351485	43.577690
3503.581246	739996.663983	43.582695
3503.242764	739945.573681	43.587700
3503.493088	739911.995511	43.592705
3503.495943	739878.408509	43.597709
3503.392338	739836.281424	43.602714
3503.495210	739785.067901	43.607719
3503.131438	739751.392375	43.612724
3503.489901	739723.484152	43.617729
3503.610605	739678.895441	43.622733
3503.451903	739628.466001	43.627738
3503.455407	739577.564312	43.632743
3503.404147	739537.455157	43.637748
3503.578134	739506.855879	43.642753
3503.555480	739458.678439	43.647757
3503.290682	739407.325192	43.652762
3503.548726	739363.355163	43.657767
3503.346461	739325.693761	43.662772
3503.251108	739281.187886	43.667777
3503.323009	739254.364078	43.672781
3503.397915	739202.409374	43.677786
3503.568602	739168.643310	43.682791
3503.201164	739121.905782	43.687796
3503.149010	739081.843944	43.692801
3503.245450	739056.054293	43.697805
3503.117224	739012.690143	43.702810
3503.440810	738967.074602	43.707815
3503.247329	738941.579704	43.712820
3503.338905	738899.316547	43.717825
3503.231181	738857.877547	43.722829
3502.822856	738816.586804	43.727834
3503.139447	738779.282563	43.732839
3503.262020	738754.724425	43.737844
3503.397352	738700.381831	43.742849
3503.718185	738669.062524	43.747853
3503.488483	738632.144443	43.752858
3503.216450	738578.362866	43.757863
3503.171609	738539.632865	43.762868
3503.594795	738498.252933	43.767873
3503.467260	738470.173031	43.772877
3503.037729	738424.431106	43.777882
3503.252826	738374.327910	43.782887
3503.284887	738332.417871	43.787892
3503.540721	738290.817065	43.792897
3503.535250	738256.779312	43.797901
3503.265673	738228.672486	43.802906
3503.445637	738184.115110	43.807911
3503.165045	738147.549494	43.812916
3503.191860	738103.462182	43.817921
3503.347052	738067.368630	43.822925
3503.117033	738036.483937	43.827930
3503.441290	738002.588675	43.832935
3503.315812	737956.695009	43.837940
3503.288554	737914.842026	43.842945
3503.599728	737853.735784	43.847949
3503.214007	737833.068331	43.852954
3503.312163	737772.342909	43.857959
3503.196443	737752.818233	43.862964
3503.191385	737708.684512	43.867969
3503.458601	737665.841611	43.872973
3503.256858	737631.635613	43.877978
3503.598199	737588.186334	43.882983
3503.145324	737553.971904	43.887988
3502.987998	737497.541716	43.892993
3503.290057	737470.822420	43.897997
3502.837915	737440.070974	43.903002
3503.090876	737394.655999	43.908007
3503.045127	737378.533026	43.913012
3503.191160	737325.614235	43.918017
3503.333327	737288.678133	43.923021
3503.245935	737254.649602	43.928026
3503.385553	737206.877133	43.933031
3503.426485	737182.228644	43.938036
3503.290211	737127.870607	43.943041
3503.313607	737092.882972	43.948045
3503.226424	737056.577376	43.953050
3503.278023	737012.826333	43.958055
3502.719270	736976.053761	43.963060
3503.120730	736945.704072	43.968065
3503.258501	736903.670145	43.973069
3503.048242	736871.590080	43.978074
3503.362479	736840.462626	43.983079
3503.162647	736803.036310	43.988084
3503.256477	736756.703735	43.993089
3503.164651	736723.514905	43.998093
3502.926771	736682.333464	44.003098
3503.177434	736639.091910	44.008103
3503.240808	736613.101870	44.013108
3503.080215	736583.833126	44.018113
3503.240768	736546.148284	44.023117
3503.086355	736516.333932	44.028122
3503.219365	736474.001617	44.033127
3502.925550	736446.040958	44.038132
3502.978007	736401.643108	44.043137
3503.205884	736374.635457	44.048141
3503.022838	736342.152889	44.053146
3503.266237	736300.444798	44.058151
3503.112446	736261.523744	44.063156
3503.086918	736229.460151	44.068161
3503.124357	736187.241043	44.073165
3502.988271	736157.422332	44.078170
3503.179961	736115.672311	44.083175
3503.126172	736086.582102	44.088180
3503.054535	736044.033791	44.093185
3503.189735	736014.714226	44.098189
3503.009787	735971.985423	44.103194
3503.079264	735939.360633	44.108199
3503.125568	735901.345157	44.113204
3503.004607	735864.940737	44.118209
3503.128009	735833.246937	44.123213
3503.147365	735796.868578	44.128218
3503.277659	735754.730872	44.133223
3503.348463	735717.155900	44.138228
3503.118296	735687.152977	44.143233
3503.508240	735654.325750	44.148237
3502.940510	735614.826372	44.153242
3503.299115	735574.283315	44.158247
3503.352555	735538.195117	44.163252
3503.014044	735504.794420	44.168257
3503.319367	735452.876337	44.173261
3503.007994	735431.596499	44.178266
3503.398770	735374.318630	44.183271
3503.442450	735338.973537	44.188276
3503.046234	735301.226103	44.193281
3503.032652	735267.721386	44.198285
3503.001555	735230.705355	44.203290
3503.254692	735185.673778	44.208295
3503.266261	735164.686478	44.213300
3503.180229	735115.206417	44.218305
3503.215940	735078.871602	44.223309
3503.008378	735060.345376	44.228314
3503.563205	735014.817679	44.233319
3503.070751	734985.053324	44.238324
3503.278196	734944.581492	44.243329
3503.180039	734904.654769	44.248333
3503.044513	734864.189548	44.253338
3503.286048	734826.285298	44.258343
3503.433578	734799.186594	44.263348
3503.140627	734749.342401	44.268353
3503.055492	734701.443539	44.273357
3503.164169	734679.647017	44.278362
3503.271366	734632.656501	44.283367
3502.826665	734603.377835	44.288372
3503.102694	734565.466672	44.293377
3503.030840	734527.167168	44.298381
3503.116556	734492.801388	44.303386
3503.045217	734464.500161	44.308391
3502.701935	734431.145275	44.313396
3502.779392	734406.680226	44.318401
3502.860546	734378.898058	44.323405
3503.022406	734335.312231	44.328410
3503.051208	734292.787583	44.333415
3502.870713	734284.204513	44.338420
3502.966152	734238.698621	44.343425
3502.988535	734214.390562	44.348429
3502.898117	734170.251408	44.353434
3502.816902	734132.743573	44.358439
3502.740508	734106.223937	44.363444
3503.083220	734073.101037	44.368449
3503.125987	734048.937623	44.373453
3502.737287	734027.567796	44.378458
3503.007473	733975.645965	44.383463
3503.082129	733947.912882	44.388468
3502.944646	733910.413282	44.393473
3503.139330	733895.481230	44.398477
3502.905003	733853.492637	44.403482
3503.187052	733812.012771	44.408487
3503.079953	733781.388412	44.413492
3503.001628	733744.076301	44.418497
3503.112465	733709.208006	44.423501
3503.146192	733678.164026	44.428506
3502.946400	733636.762651	44.433511
3503.117028	733597.527703	44.438516
3502.872398	733566.578661	44.443521
3503.116338	733533.519324	44.448525
3502.938712	733496.420444	44.453530
3502.999704	733458.688019	44.458535
3502.995911	733435.173996	44.463540
3502.928687	733395.086166	44.468545
3503.192047	733375.389346	44.473549
3503.096640	733334.563281	44.478554
3503.225159	733289.888171	44.483559
3503.002393	733267.944419	44.488564
3502.811839	733228.222621	44.493569
3503.013486	733194.574791	44.498573
3502.915005	733169.837938	44.503578
3503.083594	733117.036202	44.508583
3502.777363	733095.155238	44.513588
3502.913301	733061.121623	44.518593
3502.942347	733024.432079	44.523597
3502.762974	733005.005336	44.528602
3502.866180	732956.223426	44.533607
3502.949646	732943.882346	44.538612
3503.297421	732895.901408	44.543617
3503.304760	732855.848120	44.548621
3502.711950	732824.309986	44.553626
3502.836690	732793.198094	44.558631
3503.148737	732764.728703	44.563636
3502.727715	732726.032585	44.568641
3502.983847	732694.750136	44.573645
3502.702894	732671.477592	44.578650
3502.919694	732630.547011	44.583655
3502.800988	732606.405879	44.588660
3502.936094	732585.391499	44.593665
3502.810144	732537.932082	44.598669
3502.839865	732519.162860	44.603674
3503.393481	732476.443134	44.608679
3502.947509	732440.274802	44.613684
3502.522557	732418.312539	44.618689
3502.880702	732367.356089	44.623693
3502.638689	732357.592824	44.628698
3503.056468	732321.776754	44.633703
3503.049582	732293.803862	44.638708
3502.964880	732253.416169	44.643713
3502.855134	732222.885351	44.648717
3502.583268	732206.096073	44.653722
3502.628807	732164.993304	44.658727
3502.498326	732135.505337	44.663732
3502.734333	732116.750703	44.668737
3502.851608	732083.557766	44.673741
3502.592212	732053.100477	44.678746
3502.744949	732037.379693	44.683751
3502.553870	732002.702315	44.688756
3502.506972	731970.031099	44.693761
3502.716220	731934.990386	44.698765
3502.339551	731923.812875	44.703770
3502.712016	731893.944071	44.708775
3502.889974	731866.137300	44.713780
3502.400162	731835.321040	44.718785
3502.849124	731799.943156	44.723789
3502.590151	731775.377019	44.728794
3502.866986	731746.365184	44.733799
3502.653808	731710.551345	44.738804
3502.686183	731690.046721	44.743809
3502.503862	731665.616166	44.748813
3502.685538	731639.689601	44.753818
3502.747022	731609.375831	44.758823
3502.509348	731583.567700	44.763828
3502.675861	731555.464651	44.768833
3502.785123	731520.042486	44.773837
3502.611096	731502.641425	44.778842
3502.707518	731475.242880	44.783847
3502.686012	731451.131798	44.788852
3502.711199	731421.268958	44.793857
3502.869776	731392.126789	44.798861
3502.514658	731356.136699	44.803866
3502.802262	731337.916455	44.808871
3502.579321	731311.015637	44.813876
3502.188330	731291.817709	44.818881
3502.600793	731271.893133	44.823885
3502.439897	731240.475708	44.828890
3502.859529	731215.895092	44.833895
3503.120093	731184.754635	44.838900
3502.684065	731160.958583	44.843905
3502.705844	731128.421211	44.848909
3502.719526	731102.273013	44.853914
3502.923551	731063.713534	44.858919
3502.783355	731041.106369	44.863924
3502.856674	731004.945083	44.868929
3502.896248	730975.821026	44.873933
3502.731416	730940.243412	44.878938
3502.945870	730910.050381	44.883943
3503.035239	730880.274013	44.888948
3502.729620	730847.343774	44.893953
3503.016873	730813.325294	44.898957
3502.786884	730787.959046	44.903962
3502.784693	730758.098274	44.908967
3502.858028	730718.320656	44.913972
3502.946939	730704.588664	44.918977
3502.586349	730653.046561	44.923981
3502.669225	730648.130358	44.928986
3502.756138	730616.521116	44.933991
3502.518464	730583.529087	44.938996
3502.477103	730565.658450	44.944001
3502.768050	730541.394133	44.949005
3502.764824	730505.589892	44.954010
3502.696818	730469.300936	44.959015
3503.053676	730444.134055	44.964020
3502.654114	730414.733680	44.969025
3502.882561	730389.142076	44.974029
3502.705924	730369.163786	44.979034
3502.498885	730321.110447	44.984039
3502.647374	730298.106975	44.989044
3502.398527	730282.696581	44.994049
3502.840414	730251.175999	44.999053
3502.626419	730236.849311	45.004058
3502.665828	730200.789078	45.009063
3502.656319	730177.117952	45.014068
3502.572093	730154.300992	45.019073
3502.820164	730117.265034	45.024077
3502.844797	730091.507976	45.029082
3502.783852	730061.505747	45.034087
3502.747632	730033.232731	45.039092
3502.805160	730004.993695	45.044097
3503.054927	729963.103222	45.049101
3502.824459	729932.583662	45.054106
3503.104838	729904.406610	45.059111
3502.848993	729868.244972	45.064116
3502.515308	729844.527239	45.069121
3502.804934	729810.504172	45.074125
3502.652006	729793.145488	45.079130
3502.787013	729766.725362	45.084135
3502.762040	729733.496719	45.089140
3502.719451	729706.709441	45.094145
3502.916046	729678.099663	45.099149
3502.829582	729651.814712	45.104154
3503.003020	729608.647263	45.109159
3502.704808	729586.705948	45.114164
3502.743427	729554.456663	45.119169
3502.747462	729542.272080	45.124173
3502.685724	729495.180486	45.129178
3503.076842	729468.073315	45.134183
3503.200980	729430.361244	45.139188
3503.018129	729405.428670	45.144193
3502.835237	729371.085389	45.149197
3502.746942	729337.122616	45.154202
3503.024896	729303.148883	45.159207
3503.006170	729269.273424	45.164212
3502.878638	729236.951198	45.169217
3502.867277	729210.206670	45.174221
3502.909747	729173.101232	45.179226
3503.040197	729145.094851	45.184231
3502.930495	729121.684818	45.189236
3502.902726	729080.281314	45.194241
3503.051599	729052.122984	45.199245
3502.798450	729035.720296	45.204250
3502.939299	728988.691455	45.209255
3502.650344	728949.460199	45.214260
3502.519253	728917.632614	45.219265
3502.927995	728893.542109	45.224269
3502.567211	728876.265248	45.229274
3502.881049	728843.769670	45.234279
3502.828160	728806.133412	45.239284
3502.736193	728776.428752	45.244289
3502.605823	728750.692991	45.249293
3502.788255	728734.069323	45.254298
3502.793866	728700.880959	45.259303
3502.535076	728670.163191	45.264308
3502.390627	728646.163108	45.269313
3502.907767	728605.459951	45.274317
3502.467136	728593.545353	45.279322
3503.038050	728571.309486	45.284327
3502.891318	728540.969043	45.289332
3502.815588	728507.892366	45.294337
3502.909979	728477.363351	45.299341
3502.475142	728446.871888	45.304346
3502.642794	728414.101475	45.309351
3502.863680	728397.024966	45.314356
3502.518685	728372.809443	45.319361
3502.757151	728324.522293	45.324365
3502.809816	728305.937693	45.329370
3502.805878	728280.031005	45.334375
3502.916371	728233.597247	45.339380
3502.971796	728210.504143	45.344385
3502.954623	728175.583610	45.349389
3502.888256	728141.711314	45.354394
3502.740784	728117.066187	45.359399
3502.681647	728095.428216	45.364404
3502.726826	728076.101265	45.369409
3502.934190	728037.378287	45.374413
3502.613269	728024.700062	45.379418
3502.468455	727982.963506	45.384423
3502.601433	727967.783034	45.389428
3502.358222	727934.038091	45.394433
3502.815200	727905.775500	45.399437
3502.783802	727885.222250	45.404442
3502.770483	727859.811161	45.409447
3503.032406	727819.096604	45.414452
3502.631551	727793.947321	45.419457
3502.914121	727756.894958	45.424461
3502.890266	727721.973586	45.429466
3503.059062	727690.735814	45.434471
3502.835674	727655.698417	45.439476
3502.714835	727634.465712	45.444481
3502.941360	727606.884085	45.449485
3502.835383	727577.177367	45.454490
3502.620968	727545.853563	45.459495
3502.829713	727514.509454	45.464500
3502.604996	727493.243957	45.469505
3503.205391	727465.203921	45.474509
3502.892699	727438.750943	45.479514
3502.750067	727399.587200	45.484519
3502.921550	727375.382696	45.489524
3502.916437	727333.619803	45.494529
3503.315943	727284.655930	45.499533
3502.878713	727270.856221	45.504538
3502.982302	727235.862230	45.509543
3503.067860	727193.241456	45.514548
3502.604959	727167.060061	45.519553
3502.801706	727124.172890	45.524557
3502.465474	727102.032969	45.529562
3502.724466	727077.515904	45.534567
3502.634166	727051.817726	45.539572
3502.595743	727028.191763	45.544577
3502.707667	727003.104182	45.549581
3502.545364	726975.782674	45.554586
3502.946276	726942.323854	45.559591
3502.817878	726923.072323	45.564596
3502.822083	726889.728199	45.569601
3503.138326	726851.625751	45.574605
3502.814446	726823.834910	45.579610
3502.771153	726795.502287	45.584615
3502.551426	726761.451359	45.589620
3502.378157	726740.621334	45.594625
3502.879555	726700.902217	45.599629
3502.572882	726682.967689	45.604634
3502.471133	726647.509558	45.609639
3502.947658	726627.513556	45.614644
3502.841751	726604.888418	45.619649
3502.696883	726563.887823	45.624653
3502.916157	726537.492913	45.629658
3502.484572	726501.097558	45.634663
3502.545880	726477.255385	45.639668
3502.180970	726457.744446	45.644673
3502.829237	726413.342284	45.649677
3502.396799	726413.512754	45.654682
3502.729185	726384.918619	45.659687
3502.813243	726366.126249	45.664692
3502.506076	726337.835522	45.669697
3502.732837	726312.181876	45.674701
3502.569605	726288.227506	45.679706
3502.701796	726263.134321	45.684711
3502.937898	726222.019692	45.689716
3502.574666	726195.719664	45.694721
3503.014911	726163.737658	45.699725
3502.442785	726138.116004	45.704730
3502.697827	726111.416534	45.709735
3502.537611	726083.546661	45.714740
3502.367794	726061.079200	45.719745
3502.661575	726034.472197	45.724749
3502.770454	725997.341400	45.729754
3502.805272	725974.443583	45.734759
3502.628052	725953.067153	45.739764
3502.515299	725923.504200	45.744769
3503.039167	725896.115578	45.749773
3502.753696	725869.900792	45.754778
3502.536514	725827.421900	45.759783
3502.633880	725786.179296	45.764788
3502.664924	725783.696731	45.769793
3502.539222	725747.297175	45.774797
3502.597124	725735.147590	45.779802
3502.637426	725700.999855	45.784807
3502.862408	725663.997076	45.789812
3502.761831	725577.445686	45.794817
3502.523962	725438.934528	45.799821
3502.555449	725243.735827	45.804826
3502.438476	724991.617058	45.809831
3502.243575	724669.775371	45.814836
3501.722843	724313.827811	45.819841
3501.946190	723875.616892	45.824845
3501.742118	723411.232894	45.829850
3501.105605	722852.515050	45.834855
3500.650599	722278.114199	45.839860
3500.614226	721625.621166	45.844865
3499.922514	720916.712598	45.849869
3499.659151	720155.162373	45.854874
3498.856584	719311.807841	45.859879
3498.590053	718436.191494	45.864884
3498.061588	717501.204014	45.869889
3497.470891	716498.855729	45.874893
3496.700945	715433.359192	45.879898
3496.006167	714311.794082	45.884903
3495.299629	713128.048694	45.889908
3494.396894	711888.232787	45.894913
3493.762279	710582.813926	45.899917
3492.662647	709244.254869	45.904922
3491.535851	707824.747733	45.909927
3490.764489	706349.072858	45.914932
3489.766526	704835.330215	45.919937
3488.708440	703245.514890	45.924941
3487.421790	701617.033073	45.929946
3486.694162	699919.763726	45.934951
3485.425062	698176.270113	45.939956
3484.450732	696361.725812	45.944961
3483.267402	694495.219725	45.949965
3481.652496	692583.871013	45.954970
3480.290476	690622.813290	45.959975
3479.045438	688596.561185	45.964980
3477.305697	686526.130347	45.969985
3476.075239	684398.880194	45.974989
3474.163970	682238.127422	45.979994
3472.915475	680010.005848	45.984999
3471.239651	677746.687285	45.990004
3469.479196	675431.446923	45.995009
3468.201394	673064.754341	46.000013
3466.123360	670660.797432	46.005018
3464.210595	668200.788714	46.010023
3462.552676	665701.137627	46.015028
3460.629992	663163.949232	46.020033
3458.918858	660564.561429	46.025037
3456.900628	657943.807010	46.030042
3454.917342	655264.010573	46.035047
3452.689603	652553.500826	46.040052
3450.768900	649801.623586	46.045057
3448.542036	647011.350758	46.050061
3446.249688	644188.216685	46.055066
3444.394746	641313.862917	46.060071
3442.126858	638404.301602	46.065076
3439.893994	635461.387603	46.070081
3437.975054	632474.792547	46.075085
3435.146547	629460.009501	46.080090
3433.210675	626388.678035	46.085095
3430.778009	623305.473810	46.090100
3427.804935	620185.796721	46.095105
3425.900756	617024.746845	46.100109
3423.315003	613824.090073	46.105114
3420.583012	610605.631108	46.110119
3418.102701	607351.287027	46.115124
3415.348713	604060.119255	46.120129
3412.787621	600738.253589	46.125133
3409.881736	597390.432158	46.130138
3407.063838	594019.133202	46.135143
3404.682838	590616.150236	46.140148
3401.666262	587187.322762	46.145153
3399.224979	583726.256642	46.150157
3396.091255	580250.845344	46.155162
3393.085892	576744.957361	46.160167
3390.447626	573204.765729	46.165172
3387.087155	569647.796429	46.170177
3384.419086	566072.253753	46.175181
3381.157398	562471.447839	46.180186
3378.035513	558848.271617	46.185191
3375.316922	555207.009099	46.190196
3371.761248	551548.014178	46.195201
3368.986216	547855.693903	46.200205
3365.672962	544155.111664	46.205210
3362.343093	540430.048245	46.210215
3359.372682	536696.176793	46.215220
3355.935508	532945.667144	46.220225
3352.695382	529169.526933	46.225229
3349.464201	525373.234623	46.230234
3345.993915	521566.375199	46.235239
3342.801849	517742.959655	46.240244
3339.488862	513905.380450	46.245249
3335.984931	510062.245319	46.250253
3332.461867	506193.265343	46.255258
3328.849654	502315.185334	46.260263
3325.446405	498425.334951	46.265268
3322.065523	494530.884922	46.270273
3318.821051	490622.720789	46.275277
3315.070446	486703.738204	46.280282
3311.437526	482783.460733	46.285287
3307.969482	478827.211959	46.290292
3304.341636	474877.983629	46.295297
3300.533739	470921.818889	46.300301
3296.861873	466947.632267	46.305306
3293.239912	462980.932407	46.310311
3289.807485	458999.871589	46.315316
3285.560361	455024.596745	46.320321
3282.091507	451023.377019	46.325325
3278.394129	447039.486948	46.330330
3274.442586	443048.254218	46.335335
3271.430316	439044.471629	46.340340
3267.315903	435049.999746	46.345345
3263.675701	431031.865655	46.350349
3260.023745	427019.949183	46.355354
3256.190861	422989.827785	46.360359
3252.520975	418980.600208	46.365364
3248.225466	414963.196852	46.370369
3244.646766	410930.983708	46.375373
3240.755536	406901.437196	46.380378
3236.856215	402874.702523	46.385383
3233.042279	398841.432171	46.390388
3229.078277	394827.012580	46.395393
3225.319609	390795.194687	46.400397
3221.275107	386769.833654	46.405402
3217.437354	382757.984613	46.410407
3213.283381	378726.348955	46.415412
3209.164399	374715.508752	46.420417
3205.572282	370696.493503	46.425421
3201.601833	366696.779464	46.430426
3197.156689	362679.372215	46.435431
3193.482534	358675.033586	46.440436
3189.461101	354698.213845	46.445441
3185.625546	350701.298005	46.450445
3181.503305	346711.955437	46.455450
3177.377159	342725.296968	46.460455
3173.592745	338729.066798	46.465460
3169.449942	334757.420563	46.470465
3165.446214	330769.319662	46.475469
3161.645792	326821.603608	46.480474
3157.643406	322865.182957	46.485479
3153.542116	318901.199800	46.490484
3149.675070	314953.493010	46.495489
3145.611153	311012.680554	46.500493
3141.099602	307077.826902	46.505498
3137.377828	303153.556141	46.510503
3133.441665	299240.763066	46.515508
3129.124794	295331.215378	46.520513
3125.287718	291421.144700	46.525517
3121.119115	287536.343289	46.530522
3116.903695	283655.287243	46.535527
3113.312283	279763.593637	46.540532
3109.061284	275903.432523	46.545537
3105.196681	272031.326677	46.550541
3100.442734	268197.722993	46.555546
3096.470937	264354.302459	46.560551
3092.538574	260518.825251	46.565556
3088.305925	256702.745594	46.570561
3084.324944	252882.529868	46.575565
3080.316630	249092.339422	46.580570
3076.519928	245305.941232	46.585575
3072.461059	241527.756041	46.590580
3067.827572	237752.780300	46.595585
3063.851686	233993.200487	46.600589
3059.708952	230252.169567	46.605594
3055.875745	226510.165097	46.610599
3052.042860	222784.897757	46.615604
3047.268868	219078.876557	46.620609
3043.248045	215363.492805	46.625613
3039.206111	211692.942553	46.630618
3035.469944	207920.004808	46.635623
3031.157060	204244.438952	46.640628
3027.091898	200587.938974	46.645633
3023.351936	196948.375600	46.650637
3018.893781	193315.862539	46.655642
3014.851665	189692.094167	46.660647
3010.815187	186079.782579	46.665652
3006.549490	182482.080897	46.670657
3002.370256	178897.291498	46.675661
2998.355535	175331.848248	46.680666
2994.254938	171773.433238	46.685671
2990.514008	168228.368722	46.690676
2985.924028	164699.991196	46.695681
2982.016919	161180.054361	46.700685
2977.735491	157667.698338	46.705690
2973.507380	154167.719364	46.710695
2969.563801	150696.503113	46.715700
2965.178831	147239.943888	46.720705
2961.306045	143783.511385	46.725709
2956.778673	140354.511169	46.730714
2952.365191	136943.958780	46.735719
2948.773305	133538.739583	46.740724
2944.615628	130156.984163	46.745729
2940.694638	126772.677907	46.750733
2936.596429	123421.704397	46.755738
2932.136477	120076.041286	46.760743
2928.325634	116735.554815	46.765748
2923.751898	113420.769518	46.770753
2919.682732	110115.779406	46.775757
2915.543229	106831.224447	46.780762
2911.239616	103560.849356	46.785767
2907.107013	100309.686823	46.790772
2902.669639	97081.294779	46.795777
2898.562729	93870.954723	46.800781
2894.431200	90674.500695	46.805786
2890.205345	87505.441317	46.810791
2885.728833	84337.651822	46.815796
2881.534225	81197.259462	46.820801
2877.190859	78076.271594	46.825805
2872.850406	74976.368584	46.830810
2868.264265	71897.875496	46.835815
2863.836867	68841.028287	46.840820
2858.981764	65825.601670	46.845825
2854.547436	62813.383568	46.850829
2850.286108	59838.351321	46.855834
2844.824482	56903.839050	46.860839
2840.320792	53993.016323	46.865844
2834.657006	51128.528819	46.870849
2829.172723	48300.385971	46.875853
2822.096758	45559.298694	46.880858
2812.726809	42942.088582	46.885863
2802.455422	40442.196594	46.890868
2791.402080	38085.319591	46.895873
2779.563395	35867.055887	46.900877
2768.204196	33791.129146	46.905882
2757.424674	31894.653387	46.910887
2746.927515	30146.199155	46.915892
2736.429147	28578.355030	46.920897
2726.976146	27160.343499	46.925901
2717.808136	25886.799074	46.930906
2708.917560	24766.160146	46.935911
2701.668435	23759.377292	46.940916
2694.637559	22886.123669	46.945921
2688.199521	22101.702119	46.950925
2682.236031	21422.666202	46.955930
2677.096609	20822.449292	46.960935
2672.645680	20283.772668	46.965940
2668.243902	19815.514885	46.970945
2664.355788	19370.861235	46.975949
2661.126117	18979.408945	46.980954
2657.455585	18617.858448	46.985959
2654.691980	18275.720057	46.990964
2651.093438	17969.952420	46.995969
2648.477359	17659.444980	47.000973
2645.273376	17364.171228	47.005978
2642.615115	17078.622128	47.010983
2640.264068	16796.263817	47.015988
2637.061163	16510.623136	47.020993
2634.376780	16227.141106	47.025997
2631.635168	15956.394633	47.031002
2629.024721	15669.687758	47.036007
2626.327633	15377.512030	47.041012
2623.453317	15089.728909	47.046017
2620.854720	14785.262962	47.051021
2618.347559	14488.688258	47.056026
2615.441589	14181.526863	47.061031
2612.863633	13858.628458	47.066036
2609.454497	13546.658996	47.071041
2606.697888	13208.519064	47.076045
2603.698210	12885.695219	47.081050
2600.649187	12537.581354	47.086055
2597.702435	12200.408466	47.091060
2594.438357	11850.252960	47.096065
2591.112647	11498.797572	47.101069
2588.159050	11145.416298	47.106074
2584.829680	10779.589700	47.111079
2581.280168	10414.523328	47.116084
2577.859806	10051.706826	47.121089
2574.735618	9679.732508	47.126093
2571.539756	9331.485045	47.131098
2568.003898	8954.187531	47.136103
2565.013118	8577.680842	47.141108
2561.337698	8207.362955	47.146113
2557.987753	7829.509961	47.151117
2554.870359	7454.949901	47.156122
2550.940489	7080.926784	47.161127
2548.030844	6687.012073	47.166132
2544.163711	6323.958076	47.171137
2540.512771	5934.917633	47.176141
2536.750775	5554.427576	47.181146
2532.975431	5192.669857	47.186151
2529.714487	4806.629627	47.191156
2525.846726	4450.192093	47.196161
2522.732266	4077.619689	47.201165
2518.904440	3702.495714	47.206170
2514.952923	3344.642712	47.211175
2511.604215	2987.491834	47.216180
2507.762149	2637.571835	47.221185
2504.183635	2281.662773	47.226189
2500.364233	1935.178690	47.231194
2496.428131	1590.527004	47.236199
2492.620365	1254.879284	47.241204
2488.828606	935.056165	47.246209
2484.848120	612.358740	47.251213
2480.629470	309.364616	47.256218
2472.705081	120.057411	47.261223
2457.069701	175.425261	47.266228
2448.053396	172.782095	47.271233
2443.120842	183.563484	47.276237
2440.712616	176.805341	47.281242
2439.737558	185.987250	47.286247
2438.699404	178.254051	47.291252
2437.030627	170.104363	47.296257
2434.532417	171.164127	47.301261
2431.664954	181.463948	47.306266
2427.894765	179.584116	47.311271
2424.711317	171.678534	47.316276
2421.145235	164.272241	47.321281
2417.902469	172.543388	47.326285
2414.668788	176.042527	47.331290
2410.849657	179.172979	47.336295
2408.021691	169.860894	47.341300
2404.405582	173.612021	47.346305
2400.906589	176.827379	47.351309
2397.932602	173.869893	47.356314
2394.326529	175.908429	47.361319
2391.506524	178.641697	47.366324
2387.410958	182.532764	47.371329
2384.545440	176.551883	47.376333
2381.253833	173.525869	47.381338
2377.423703	191.025747	47.386343
2374.646104	180.341738	47.391348
2370.981526	174.359173	47.396353
2367.456051	172.803284	47.401357
2364.153549	166.330755	47.406362
2360.152649	175.551970	47.411367
2357.065306	169.361250	47.416372
2353.996566	170.771779	47.421377
2350.798579	176.909625	47.426381
2346.925817	179.129569	47.431386
2342.954607	175.253145	47.436391
2340.209348	171.724131	47.441396
2336.505809	173.971994	47.446401
2332.848651	168.397521	47.451405
2329.437639	167.191001	47.456410
2326.074783	168.004009	47.461415
2323.431224	166.445238	47.466420
2320.198871	170.144121	47.471425
2316.084209	167.185751	47.476429
2312.627431	156.445792	47.481434
2309.234747	171.497693	47.486439
2305.617421	165.635458	47.491444
2301.911251	167.557773	47.496449
2298.742974	169.120143	47.501453
2295.498281	165.608488	47.506458
2291.751117	173.364249	47.511463
2288.709205	159.375677	47.516468
2284.436610	170.760049	47.521473
2280.655583	163.865340	47.526477
2278.255563	166.767718	47.531482
2273.968419	172.146281	47.536487
2271.106551	162.449156	47.541492
2267.932389	155.018149	47.546497
2264.349672	164.859498	47.551501
2260.858466	159.330112	47.556506
2257.185107	161.599492	47.561511
2253.515100	158.494947	47.566516
2250.195081	157.645448	47.571521
2246.384161	161.402403	47.576525
2243.345039	160.895094	47.581530
2239.713819	164.577194	47.586535
2236.476764	160.750550	47.591540
2232.906490	164.462455	47.596545
2229.323926	161.244624	47.601549
2225.976528	156.971273	47.606554
2222.022252	167.001478	47.611559
2218.796687	164.517427	47.616564
2215.217342	160.636210	47.621569
2211.846696	162.355977	47.626573
2208.766313	156.035157	47.631578
2204.732123	162.449484	47.636583
2201.527848	152.755667	47.641588
2198.106320	162.605963	47.646593
2194.397897	162.707873	47.651597
2191.099023	158.958564	47.656602
2187.518601	166.086948	47.661607
2183.995174	156.093981	47.666612
2180.236637	159.337540	47.671617
2176.958468	154.689097	47.676621
2173.920648	153.471983	47.681626
2170.354802	163.526889	47.686631
2166.999537	172.289187	47.691636
2163.279533	161.792124	47.696641
2159.465094	167.252177	47.701645
2156.229752	160.429883	47.706650
2152.307438	167.294856	47.711655
2149.157164	153.219898	47.716660
2145.575418	160.093958	47.721665
2142.498834	161.889342	47.726669
2138.816987	160.157368	47.731674
2134.973706	161.789465	47.736679
2132.008320	156.922457	47.741684
2128.273229	158.859937	47.746689
2124.756330	153.289711	47.751693
2121.566315	155.857480	47.756698
2117.753978	161.040346	47.761703
2114.284895	150.041902	47.766708
2110.645798	152.877621	47.771713
2107.221517	153.770384	47.776717
2104.155898	152.244136	47.781722
2100.306640	149.054659	47.786727
2096.878900	150.220724	47.791732
2093.169137	150.307343	47.796737
2089.784593	152.327865	47.801741
2086.195998	147.372582	47.806746
2082.672507	152.227353	47.811751
2079.519849	149.578029	47.816756
2076.038977	150.002400	47.821761
2072.540991	157.497516	47.826765
2068.905928	149.758155	47.831770
2064.866078	148.993320	47.836775
2062.115014	150.824786	47.841780
2058.635066	148.645911	47.846785
2054.597701	155.328073	47.851789
2051.545783	151.817911	47.856794
2047.901356	155.050024	47.861799
2044.623491	134.555469	47.866804
2041.174498	148.822895	47.871809
2037.420212	145.058134	47.876813
2034.245480	145.652800	47.881818
2030.556171	144.246571	47.886823
2027.026416	144.105385	47.891828
2023.472445	152.625483	47.896833
2019.889525	155.524019	47.901837
2016.371440	144.917381	47.906842
2012.911599	148.894973	47.911847
2009.213705	143.317831	47.916852
2006.162279	139.830711	47.921857
2002.361005	142.948253	47.926861
1999.113469	135.147127	47.931866
1995.091938	151.519236	47.936871
1991.838283	139.444555	47.941876
1988.577832	146.036145	47.946881
1984.958804	153.752001	47.951885
1981.713880	140.437186	47.956890
1978.219427	146.924359	47.961895
1974.572316	138.950265	47.966900
1971.049573	142.566090	47.971905
1967.266483	139.889735	47.976909
1964.289305	134.869488	47.981914
1960.421399	143.948436	47.986919
1957.318468	143.502170	47.991924
1953.593633	155.076141	47.996929
1949.629517	148.164403	48.001933
1946.571772	143.963997	48.006938
1943.186814	153.408197	48.011943
1939.695095	139.948877	48.016948
1935.851508	137.379236	48.021953
1932.327341	151.885294	48.026957
1929.129304	136.047297	48.031962
1925.423409	145.212390	48.036967
1922.150706	146.267720	48.041972
1918.708254	145.568524	48.046977
1915.070643	152.587928	48.051981
1911.989408	138.759497	48.056986
1908.378640	144.710220	48.061991
1904.689564	140.634053	48.066996
1901.081073	143.632605	48.072001
1897.184250	141.155856	48.077005
1894.132664	129.344684	48.082010
1890.464852	147.398567	48.087015
1887.038767	138.021466	48.092020
1883.510124	147.006346	48.097025
1879.825271	146.856945	48.102029
1876.727036	144.011693	48.107034
1873.085327	146.842490	48.112039
1869.715486	137.338499	48.117044
1866.059339	137.199365	48.122049
1862.603083	139.457642	48.127053
1859.191225	140.969949	48.132058
1855.596399	141.511577	48.137063
1852.054657	146.502526	48.142068
1848.796760	139.260313	48.147073
1844.704187	142.603698	48.152077
1841.834994	133.655425	48.157082
1838.115238	138.163297	48.162087
1834.598520	130.386834	48.167092
1830.922149	135.380695	48.172097
1827.450881	133.092815	48.177101
1824.130600	125.251353	48.182106
1820.218930	133.790405	48.187111
1817.122320	133.738457	48.192116
1813.428052	131.589450	48.197121
1809.951081	140.795344	48.202125
1806.885768	131.976387	48.207130
1803.366235	144.835942	48.212135
1799.605623	132.523704	48.217140
1796.321548	130.495999	48.222145
1792.568010	136.460320	48.227149
1789.020821	130.855512	48.232154
1785.185246	137.742136	48.237159
1782.252277	130.917743	48.242164
1778.744841	140.299782	48.247169
1775.059753	134.428070	48.252173
1771.773283	130.992767	48.257178
1767.773928	135.177660	48.262183
1764.355793	137.786694	48.267188
1760.969471	134.496756	48.272193
1757.426592	142.266487	48.277197
1754.041949	131.893197	48.282202
1750.836835	137.306161	48.287207
1747.393179	138.586400	48.292212
1743.612011	124.745084	48.297217
1740.287903	140.750724	48.302221
1736.856268	126.053827	48.307226
1732.942665	138.992732	48.312231
1729.563521	141.392091	48.317236
1725.991021	124.982685	48.322241
1722.361709	146.723298	48.327245
1719.283533	130.584278	48.332250
1715.256965	137.044682	48.337255
1712.146304	138.211125	48.342260
1708.462673	141.799645	48.347265
1704.885485	135.783079	48.352269
1701.548905	129.808860	48.357274
1697.865313	139.431206	48.362279
1694.615969	132.510745	48.367284
1691.245254	139.716498	48.372289
1687.615465	137.379925	48.377293
1684.326688	132.875887	48.382298
1680.424247	143.097214	48.387303
1677.137794	135.328814	48.392308
1673.902058	138.320411	48.397313
1670.057830	142.724849	48.402317
1666.378677	138.796230	48.407322
1662.829415	143.226334	48.412327
1659.337750	133.518469	48.417332
1656.195966	127.964006	48.422337
1652.555733	145.532753	48.427341
1649.101273	129.766376	48.432346
1645.659709	133.701532	48.437351
1642.245398	138.308270	48.442356
1639.060601	137.833905	48.447361
1634.955787	146.207280	48.452365
1631.654595	135.818918	48.457370
1627.864157	138.953309	48.462375
1624.201884	134.068398	48.467380
1621.066768	136.750948	48.472385
1617.603572	134.965304	48.477389
1614.164110	130.043192	48.482394
1610.221261	133.653698	48.487399
1606.600346	129.287284	48.492404
1603.240476	128.302942	48.497409
1599.658950	131.561494	48.502413
1597.003721	121.535113	48.507418
1593.312357	119.997752	48.512423
1589.758741	131.181737	48.517428
1586.187693	127.353530	48.522433
1582.415343	121.286833	48.527437
1579.030170	119.845313	48.532442
1575.247238	123.708062	48.537447
1571.832479	116.578428	48.542452
1568.496469	123.148812	48.547457
1564.784129	123.711461	48.552461
1561.509271	127.480595	48.557466
1557.973914	131.369740	48.562471
1554.486881	128.176524	48.567476
1551.202871	119.932638	48.572481
1547.461021	121.360176	48.577485
1544.253441	121.013965	48.582490
1540.351031	128.228934	48.587495
1536.709996	127.273737	48.592500
1533.279256	124.456045	48.597505
1529.931749	133.918376	48.602509
1526.619023	124.955415	48.607514
1522.707542	127.925969	48.612519
1519.486678	130.677417	48.617524
1516.059840	126.149356	48.622529
1512.133970	128.072063	48.627533
1508.752431	118.193201	48.632538
1505.251619	124.534914	48.637543
1502.094875	130.629537	48.642548
1498.809538	125.511350	48.647553
1495.303796	131.997944	48.652557
1491.806243	122.551689	48.657562
1487.957617	126.629015	48.662567
1484.309992	119.197723	48.667572
1480.949386	125.980224	48.672577
1477.210163	136.865010	48.677581
1473.808857	126.334078	48.682586
1470.115849	135.998786	48.687591
1466.744109	129.184572	48.692596
1463.534670	125.316240	48.697601
1459.640321	138.136514	48.702605
1456.463167	123.699148	48.707610
1453.037081	129.710439	48.712615
1449.461158	121.273336	48.717620
1446.171047	124.111461	48.722625
1442.177882	128.162982	48.727629
1438.994950	129.554278	48.732634
1435.507820	125.786919	48.737639
1432.245326	129.949759	48.742644
1428.471771	125.246605	48.747649
1424.896752	136.399901	48.752653
1421.637613	124.085657	48.757658
1417.863884	130.577522	48.762663
1414.130968	124.131881	48.767668
1410.665189	124.471166	48.772673
1406.934197	132.534285	48.777677
1404.013603	119.227146	48.782682
1400.684752	130.380024	48.787687
1397.154682	120.457327	48.792692
1393.291858	125.051730	48.797697
1389.845999	123.364237	48.802701
1386.622251	124.561227	48.807706
1382.615772	132.615629	48.812711
1379.422196	121.317139	48.817716
1376.109412	126.209597	48.822721
1372.450623	124.983955	48.827725
1368.975338	128.375883	48.832730
1365.176952	131.489098	48.837735
1361.602588	128.323493	48.842740
1358.263514	123.128653	48.847745
1354.824107	113.648440	48.852749
1351.620049	124.173508	48.857754
1347.679340	125.079161	48.862759
1344.227034	128.362128	48.867764
1340.763184	127.814113	48.872769
1337.288996	130.953488	48.877773
1333.930936	125.978481	48.882778
1330.043328	135.347674	48.887783
1326.523243	125.242229	48.892788
1323.171010	119.874750	48.897793
1319.885321	132.949125	48.902797
1316.563569	118.302926	48.907802
1313.078590	133.427234	48.912807
1309.131806	128.470231	48.917812
1305.629457	126.330764	48.922817
1302.245411	123.945201	48.927821
1299.033800	119.715237	48.932826
1295.411094	118.605254	48.937831
1291.746844	119.929393	48.942836
1288.288163	132.887142	48.947841
1284.652092	132.791717	48.952845
1281.430768	132.968144	48.957850
1277.933402	129.974191	48.962855
1274.267662	129.426251	48.967860
1270.798441	134.392201	48.972865
1267.152077	124.429242	48.977869
1263.841382	117.694895	48.982874
1260.165842	121.565197	48.987879
1256.567456	129.547894	48.992884
1252.989224	111.129029	48.997889
1249.668323	122.428090	49.002893
1246.664617	121.013941	49.007898
1242.765701	122.526297	49.012903
1239.355566	118.810700	49.017908
1235.928727	119.737271	49.022913
1232.243141	123.117293	49.027917
1228.675619	120.434539	49.032922
1224.915815	118.914911	49.037927
1222.012665	117.227223	49.042932
1218.104272	123.852401	49.047937
1214.574667	130.858975	49.052941
1211.490703	122.702664	49.057946
1207.706566	118.683453	49.062951
1204.135628	124.492909	49.067956
1200.779516	114.632206	49.072961
1197.282602	118.811459	49.077965
1193.631992	113.770673	49.082970
1190.083193	127.256454	49.087975
1186.935305	120.766787	49.092980
1183.672060	115.996060	49.097985
1179.455302	119.471438	49.102989
1176.222472	118.144355	49.107994
1172.704494	126.485402	49.112999
1169.244291	122.936204	49.118004
1165.618798	115.946530	49.123009
1162.078494	116.195117	49.128013
1158.871069	112.169010	49.133018
1155.171090	115.305589	49.138023
1151.665088	112.562604	49.143028
1148.123743	118.026009	49.148033
1144.495310	118.956772	49.153037
1141.674945	111.901692	49.158042
1137.829150	116.110845	49.163047
1133.784284	117.535138	49.168052
1130.703074	112.469924	49.173057
1127.038391	123.337097	49.178061
1123.763209	110.242735	49.183066
1119.872301	114.540467	49.188071
1116.503634	114.686315	49.193076
1113.422632	114.825254	49.198081
1109.419306	121.787676	49.203085
1105.964759	107.349326	49.208090
1102.260993	117.964857	49.213095
1099.046808	116.082203	49.218100
1095.991747	116.619827	49.223105
1092.105318	114.807680	49.228109
1088.927092	119.112316	49.233114
1085.357849	120.562992	49.238119
1081.591406	111.320416	49.243124
1077.918325	118.025395	49.248129
1074.395322	118.498916	49.253133
1071.367054	112.932833	49.258138
1067.410646	114.081481	49.263143
1064.098096	120.435982	49.268148
1060.493693	117.380379	49.273153
1057.187486	116.170105	49.278157
1053.890684	113.343272	49.283162
1049.915487	116.535704	49.288167
1046.612521	116.821111	49.293172
1043.242699	110.125335	49.298177
1039.203557	127.275537	49.303181
1036.411932	113.938288	49.308186
1032.576620	115.754858	49.313191
1028.877358	117.115977	49.318196
1025.584943	121.864207	49.323201
1021.800688	122.881022	49.328205
1018.557314	110.355940	49.333210
1015.000690	115.325469	49.338215
1011.665750	107.729424	49.343220
1008.223623	110.877943	49.348225
1004.338906	118.062376	49.353229
1001.021324	119.354481	49.358234
997.391061	119.404357	49.363239
993.859791	109.667323	49.368244
990.626288	110.128162	49.373249
987.156540	125.766178	49.378253
983.837803	110.730636	49.383258
979.719248	117.561649	49.388263
976.383570	120.610103	49.393268
973.287804	121.405948	49.398273
969.377646	120.480126	49.403277
966.210213	116.497279	49.408282
962.625641	111.562201	49.413287
958.760844	110.890557	49.418292
955.604747	109.948580	49.423297
951.972936	115.602915	49.428301
948.291822	113.147368	49.433306
944.856393	114.278045	49.438311
941.341486	112.354861	49.443316
938.036646	109.706655	49.448321
934.241070	112.472635	49.453325
931.122742	106.789928	49.458330
927.545726	113.257521	49.463335
923.989248	111.853709	49.468340
920.341734	116.896554	49.473345
916.949798	114.812154	49.478349
913.887039	107.340293	49.483354
909.819320	109.744787	49.488359
906.095019	107.861197	49.493364
902.901958	106.592070	49.498369
899.376540	114.308381	49.503373
896.114389	113.798788	49.508378
892.753617	119.182195	49.513383
888.629060	110.927695	49.518388
885.701262	109.361526	49.523393
881.867700	111.865256	49.528397
878.516399	99.936350	49.533402
874.783671	114.551907	49.538407
871.599648	109.765165	49.543412
867.854583	111.007102	49.548417
864.293148	110.103619	49.553421
860.979854	102.292971	49.558426
857.402891	109.947386	49.563431
853.889817	104.512566	49.568436
850.376925	104.208861	49.573441
847.076824	110.696226	49.578445
843.646172	101.790447	49.583450
840.100866	108.508605	49.588455
836.438284	111.543344	49.593460
833.239102	105.561308	49.598465
829.205826	120.909003	49.603469
825.750952	111.493574	49.608474
822.359439	119.877682	49.613479
818.499497	111.927586	49.618484
815.327824	108.117239	49.623489
811.679197	113.752952	49.628493
808.781735	111.195331	49.633498
805.104513	108.978237	49.638503
801.502626	107.221504	49.643508
797.978968	107.954848	49.648513
794.056825	113.011839	49.653517
791.129594	101.088837	49.658522
787.288135	114.181836	49.663527
783.912813	113.767021	49.668532
780.588160	105.716185	49.673537
776.622390	111.799846	49.678541
773.256786	103.072417	49.683546
769.866188	102.772030	49.688551
766.159796	110.347477	49.693556
762.669913	106.894495	49.698561
759.150378	112.031931	49.703565
755.720561	108.961718	49.708570
752.637489	110.519109	49.713575
748.955414	104.274642	49.718580
745.660083	100.315096	49.723585
741.524362	111.478706	49.728589
738.163587	110.581598	49.733594
734.604496	108.182418	49.738599
731.072457	114.018738	49.743604
727.950292	109.015855	49.748609
724.114058	105.690453	49.753613
720.569322	100.108248	49.758618
717.323161	105.755793	49.763623
713.436661	112.982586	49.768628
710.469843	102.900436	49.773633
706.735054	108.379785	49.778637
703.324858	100.888014	49.783642
699.575874	104.675191	49.788647
696.166949	97.073105	49.793652
692.857460	103.556993	49.798657
689.234642	116.948182	49.803661
685.997074	96.333826	49.808666
682.259787	107.031763	49.813671
678.558480	115.322966	49.818676
675.290766	107.311540	49.823681
671.580584	113.067262	49.828685
668.581535	104.282436	49.833690
665.066309	104.149764	49.838695
660.948118	106.394306	49.843700
657.919141	103.923471	49.848705
654.339356	106.954918	49.853709
650.995604	114.890587	49.858714
647.307904	107.416750	49.863719
643.648034	109.071026	49.868724
640.317275	100.197247	49.873729
636.342926	103.713128	49.878733
633.042882	101.932053	49.883738
629.571730	110.216785	49.888743
625.931955	106.048311	49.893748
622.935626	108.449654	49.898753
618.988811	107.740374	49.903757
615.637599	98.650760	49.908762
611.880756	102.760572	49.913767
608.485465	101.477564	49.918772
605.122025	95.663393	49.923777
601.624761	106.982554	49.928781
598.525685	95.364413	49.933786
594.786425	108.194757	49.938791
591.493911	103.893081	49.943796
588.080474	97.509791	49.948801
583.942066	112.452167	49.953805
580.471797	104.198461	49.958810
577.004951	94.874440	49.963815
573.515278	101.800457	49.968820
570.477059	105.533085	49.973825
566.855304	110.892808	49.978829
563.146446	102.739967	49.983834
559.505006	108.170835	49.988839
555.897054	107.875596	49.993844
552.766565	106.285965	49.998849
548.810259	112.587491	50.003853
545.908836	113.174267	50.008858
542.277563	104.228144	50.013863
538.806407	98.261550	50.018868
535.122665	96.410841	50.023873
531.516255	97.271361	50.028877
528.098630	105.431665	50.033882
524.685170	107.865589	50.038887
520.997070	108.903818	50.043892
517.471573	106.883672	50.048897
514.017639	109.880196	50.053901
510.607584	96.352070	50.058906
506.901691	104.926346	50.063911
503.341593	104.631126	50.068916
500.346570	101.678616	50.073921
496.505505	100.440060	50.078925
493.039514	98.773975	50.083930
489.282790	94.853099	50.088935
485.898069	96.090585	50.093940
482.743032	98.990112	50.098945
479.072843	102.129206	50.103949
475.613390	101.183710	50.108954
472.486601	100.350506	50.113959
468.630158	100.269328	50.118964
465.125918	104.835730	50.123969
461.204779	113.123613	50.128973
457.935517	105.636947	50.133978
454.515807	111.298594	50.138983
451.252674	108.017918	50.143988
447.626729	102.018802	50.148993
443.787379	107.165197	50.153997
440.506271	101.462646	50.159002
436.898705	102.728959	50.164007
433.580278	112.908630	50.169012
429.903809	94.295919	50.174017
426.214392	103.270093	50.179021
423.056335	97.650203	50.184026
419.690458	107.386624	50.189031
415.729673	109.048657	50.194036
412.556825	99.696451	50.199041
408.529725	111.244134	50.204045
405.529556	99.511904	50.209050
401.845727	105.131655	50.214055
398.653338	110.074321	50.219060
395.672647	97.284119	50.224065
391.451839	99.839526	50.229069
387.877116	100.151656	50.234074
384.711083	96.306372	50.239079
380.645352	100.893740	50.244084
377.508091	99.468951	50.249089
374.119494	102.203757	50.254093
370.491655	94.962604	50.259098
366.964401	99.612415	50.264103
363.022536	105.032971	50.269108
360.113211	100.846057	50.274113
356.377738	101.297496	50.279117
353.053923	94.114576	50.284122
349.661788	98.613767	50.289127
346.098216	108.007628	50.294132
342.523873	98.118482	50.299137
338.508340	103.261564	50.304141
335.230257	100.334713	50.309146
332.011732	105.907104	50.314151
328.676356	105.104386	50.319156
325.171541	92.742191	50.324161
321.116812	97.197944	50.329165
317.861115	100.085830	50.334170
314.293229	99.397189	50.339175
310.831603	101.622771	50.344180
307.557126	96.112622	50.349185
303.492919	102.908382	50.354189
300.175161	99.944515	50.359194
297.185579	101.133714	50.364199
293.547971	102.667376	50.369204
290.188200	99.771448	50.374209
286.297067	92.463646	50.379213
282.759907	105.927952	50.384218
279.581334	91.515754	50.389223
275.534598	108.701499	50.394228
272.467890	101.411161	50.399233
268.499436	111.174418	50.404237
265.403527	99.176357	50.409242
261.908245	101.542329	50.414247
258.053043	108.315374	50.419252
254.819188	101.207626	50.424257
251.063295	105.490049	50.429261
248.113938	102.247974	50.434266
244.668413	99.062580	50.439271
240.676300	102.272526	50.444276
237.377460	102.413605	50.449281
233.984536	94.440059	50.454285
230.355692	96.728116	50.459290
226.811509	104.650877	50.464295
223.291839	100.029138	50.469300
219.999938	96.726573	50.474305
216.043666	110.033966	50.479309
212.762913	96.611206	50.484314
209.076437	104.008747	50.489319
205.679521	98.933157	50.494324
202.199147	95.118151	50.499329
198.780677	104.504672	50.504333
195.438276	100.026476	50.509338
191.962707	105.727358	50.514343
188.041927	98.238670	50.519348
185.036984	93.020656	50.524353
181.171051	96.751054	50.529357
177.723584	96.630058	50.534362
174.521724	92.782978	50.539367
170.685844	92.135075	50.544372
167.019020	90.485341	50.549377
163.864400	96.638087	50.554381
160.145559	93.075323	50.559386
156.947907	89.591052	50.564391
153.483040	97.378583	50.569396
150.023041	86.378645	50.574401
146.136193	104.120940	50.579405
142.666679	88.087386	50.584410
139.281901	94.614906	50.589415
135.354010	91.736600	50.594420
132.474400	87.888692	50.599425
128.521367	90.073231	50.604429
125.172974	83.481847	50.609434
121.774574	77.585276	50.614439
118.219958	86.968534	50.619444
114.743324	79.867367	50.624449
111.094509	87.459629	50.629453
107.772695	80.778613	50.634458
104.144345	84.134863	50.639463
100.632862	89.171607	50.644468
97.510723	88.426514	50.649473
93.200463	87.139718	50.654477
89.888614	86.038872	50.659482
86.762405	88.879241	50.664487
83.136335	91.858421	50.669492
80.028936	84.936302	50.674497
76.037789	86.109544	50.679501
72.812780	86.970441	50.684506
69.363141	89.301182	50.689511
65.477922	99.518699	50.694516
61.885149	85.830437	50.699521
58.514991	89.740911	50.704525
54.993633	85.903219	50.709530
52.125182	89.271032	50.714535
48.153358	87.098255	50.719540
44.768004	92.223285	50.724545
41.418541	94.067410	50.729549
37.597882	94.077391	50.734554
33.929069	87.951570	50.739559
30.455263	87.648772	50.744564
27.606020	79.485736	50.749569
23.852506	84.052112	50.754573
20.037217	74.606537	50.759578
16.276791	88.622038	50.764583
12.774725	89.806705	50.769588
9.465336	82.715824	50.774593
6.135474	96.834485	50.779597
2.981461	87.234226	50.784602