Tue Jun 21 10:49:36 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.067822	113.515807	0.000000
-0.424645	112.733348	0.005005
-0.134109	101.097837	0.010010
-0.094012	93.259275	0.015014
-0.279544	99.261822	0.020019
-0.452963	82.755776	0.025024
-0.833791	83.496768	0.030029
-1.107859	61.554276	0.035034
-1.335285	56.544022	0.040038
-1.639895	53.384123	0.045043
-1.825903	41.247405	0.050048
-2.450472	34.687546	0.055053
-2.366131	20.234964	0.060058
-2.941297	25.144443	0.065062
-3.292379	13.115199	0.070067
-3.455610	8.992197	0.075072
-3.614850	19.283347	0.080077
-3.589454	2.065837	0.085082
-4.082337	-2.276670	0.090086
-4.286695	0.606354	0.095091
-5.034216	-1.877338	0.100096
-5.583860	0.501647	0.105101
-5.983207	2.146529	0.110106
-6.049990	-0.725758	0.115110
-6.357622	7.740154	0.120115
-5.771125	1.633535	0.125120
-6.231986	4.088986	0.130125
-6.193877	-4.576022	0.135130
-7.284866	2.166645	0.140134
-7.887309	4.632715	0.145139
-7.615020	4.961266	0.150144
-7.739459	6.007106	0.155149
-7.772755	2.588975	0.160154
-7.897998	10.608116	0.165158
-8.181885	7.078151	0.170163
-9.062125	-1.770848	0.175168
-9.492523	1.218674	0.180173
-9.294995	-8.265221	0.185178
-9.295451	4.097079	0.190182
-9.752194	2.246432	0.195187
-9.582198	0.910050	0.200192
-9.897264	0.829110	0.205197
-10.430219	0.324464	0.210202
-10.701015	2.861317	0.215206
-10.945291	-5.691612	0.220211
-10.865283	1.120193	0.225216
-11.445183	5.574808	0.230221
-12.110752	-3.706968	0.235226
-12.510361	3.473155	0.240230
-12.344330	-0.810138	0.245235
-12.421663	-6.555230	0.250240
-12.894330	-6.644211	0.255245
-12.668172	-10.599228	0.260250
-12.552368	-6.874315	0.265254
-13.226763	-9.170017	0.270259
-14.026434	-0.670583	0.275264
-14.135237	6.421919	0.280269
-13.956093	-3.027164	0.285274
-14.026596	2.618462	0.290278
-14.886984	3.697567	0.295283
-15.148366	3.170842	0.300288
-15.388708	-3.340538	0.305293
-15.323282	-7.364646	0.310298
-15.625399	-1.475442	0.315302
-15.660169	6.933644	0.320307
-16.251048	-2.322218	0.325312
-16.794262	-2.278156	0.330317
-16.796622	-5.253857	0.335322
-16.482560	-0.148670	0.340326
-16.888387	-0.475257	0.345331
-17.779560	0.278610	0.350336
-18.265196	2.280352	0.355341
-18.407051	2.234469	0.360346
-18.491815	10.309658	0.365350
-18.751984	11.468551	0.370355
-18.760377	0.052915	0.375360
-18.501684	6.889401	0.380365
-18.321537	-6.323584	0.385370
-19.369447	0.158575	0.390374
-20.041546	12.008527	0.395379
-19.944169	-1.108863	0.400384
-20.360515	0.449048	0.405389
-20.059947	4.252098	0.410394
-21.039874	0.451609	0.415398
-21.732484	1.510234	0.420403
-21.341528	2.298850	0.425408
-22.150825	6.900578	0.430413
-21.714825	5.290846	0.435418
-21.779336	4.738821	0.440422
-22.137200	3.045850	0.445427
-21.905273	-6.471961	0.450432
-22.653567	7.357425	0.455437
-23.178957	1.525502	0.460442
-23.421613	4.291339	0.465446
-23.677581	0.055629	0.470451
-23.409027	-6.141603	0.475456
-23.754918	-1.036455	0.480461
-24.167808	-8.217621	0.485466
-24.426500	-1.611000	0.490470
-24.925618	-3.446340	0.495475
-24.982421	3.504153	0.500480
-25.314491	3.017747	0.505485
-25.213813	-1.998669	0.510490
-25.695690	-0.864828	0.515494
-26.180859	9.094104	0.520499
-26.634073	0.047709	0.525504
-26.907958	8.901910	0.530509
-26.558545	-3.462354	0.535514
-26.569593	-1.904267	0.540518
-27.274198	-3.094438	0.545523
-27.730704	-4.910786	0.550528
-28.116702	9.510596	0.555533
-28.060416	-8.160552	0.560538
-28.154726	1.598675	0.565542
-28.055086	1.668695	0.570547
-28.007373	-7.809137	0.575552
-29.500463	3.925754	0.580557
-29.463915	2.094654	0.585562
-29.572213	-2.432501	0.590566
-29.869187	-0.462394	0.595571
-29.329414	-6.858853	0.600576
-30.021489	-8.475364	0.605581
-30.769093	0.525950	0.610586
-31.252016	-2.165931	0.615590
-31.577448	-3.101579	0.620595
-30.823055	-5.768856	0.625600
-31.246170	-5.741326	0.630605
-31.524020	6.255271	0.635610
-32.293126	-10.009747	0.640614
-32.670388	-3.694489	0.645619
-32.565684	-6.187087	0.650624
-33.235069	-4.124921	0.655629
-33.022787	-5.316359	0.660634
-33.047219	-2.018735	0.665638
-33.245833	6.277373	0.670643
-33.425668	-9.402059	0.675648
-34.396238	-2.651505	0.680653
-34.845503	-7.419181	0.685658
-34.761405	2.128956	0.690662
-34.813948	-5.999289	0.695667
-34.830902	-6.360473	0.700672
-34.755177	-3.303606	0.705677
-35.516003	-4.923137	0.710682
-35.897915	-0.181826	0.715686
-36.157776	-9.036851	0.720691
-36.177081	-7.113516	0.725696
-36.110990	-6.083638	0.730701
-36.930449	-7.075411	0.735706
-37.666540	-6.520085	0.740710
-37.705516	-10.592024	0.745715
-37.819784	-15.973229	0.750720
-38.247978	-2.469376	0.755725
-37.912589	-6.725656	0.760730
-37.935706	7.046591	0.765734
-38.302364	-2.046497	0.770739
-37.930393	5.394207	0.775744
-38.704561	-1.557228	0.780749
-39.077516	-3.024515	0.785754
-39.154962	-0.908820	0.790758
-40.049136	4.569311	0.795763
-40.299911	0.175863	0.800768
-40.934168	-1.717411	0.805773
-41.029011	0.869634	0.810778
-40.899578	3.092756	0.815782
-40.958746	5.004934	0.820787
-41.014543	-1.385846	0.825792
-41.290437	2.235409	0.830797
-41.256559	-4.822801	0.835802
-41.834219	5.023179	0.840806
-42.456019	3.123896	0.845811
-42.327836	-0.432665	0.850816
-42.530266	0.557813	0.855821
-43.411363	0.312300	0.860826
-43.508598	-1.784948	0.865830
-44.518067	6.458760	0.870835
-44.036027	-1.709863	0.875840
-44.315222	6.282673	0.880845
-44.158759	-2.407459	0.885850
-43.863255	3.888745	0.890854
-44.072043	2.369606	0.895859
-44.615740	-5.987708	0.900864
-45.435410	-2.441967	0.905869
-45.436696	-0.969956	0.910874
-45.543906	2.778469	0.915878
-46.279783	-3.646110	0.920883
-46.515836	-9.556525	0.925888
-46.987533	3.731353	0.930893
-47.110337	-2.130133	0.935898
-46.970642	0.517923	0.940902
-47.470918	-2.019333	0.945907
-47.168786	-11.527256	0.950912
-47.781164	4.928422	0.955917
-48.452394	-4.506524	0.960922
-48.552777	2.964447	0.965926
-48.815562	7.199015	0.970931
-48.719615	-1.857015	0.975936
-49.193826	7.898428	0.980941
-49.024015	-1.205354	0.985946
-48.851132	4.212105	0.990950
-49.879369	-0.609666	0.995955
-50.091225	-7.377356	1.000960
-50.659741	1.124058	1.005965
-50.357318	2.674042	1.010970
-50.566721	4.016731	1.015974
-51.359057	8.698535	1.020979
-51.870225	2.866828	1.025984
-52.489123	4.936028	1.030989
-51.633437	4.303843	1.035994
-51.966520	-2.558622	1.040998
-52.431049	-4.583008	1.046003
-52.197463	-4.531224	1.051008
-52.493920	9.500790	1.056013
-52.694249	0.933875	1.061018
-53.437471	-2.305318	1.066022
-53.846183	2.192977	1.071027
-53.973551	-3.778653	1.076032
-53.795856	0.413753	1.081037
-53.791218	3.455950	1.086042
-54.445077	8.967894	1.091046
-54.857395	6.468759	1.096051
-54.928231	-4.615072	1.101056
-55.132689	2.987587	1.106061
-55.630212	-3.046276	1.111066
-56.375031	-7.042567	1.116070
-56.987981	2.018936	1.121075
-55.856810	-4.080006	1.126080
-56.677608	2.534454	1.131085
-56.780201	-5.175640	1.136090
-56.911671	-3.328449	1.141094
-56.984418	1.267932	1.146099
-57.566262	0.596551	1.151104
-58.182958	3.514315	1.156109
-58.403077	1.931144	1.161114
-58.299660	-0.871844	1.166118
-58.629871	7.109407	1.171123
-58.775084	-1.220756	1.176128
-58.782577	0.387654	1.181133
-59.241576	-0.717878	1.186138
-59.749130	-4.638416	1.191142
-60.418573	-0.088458	1.196147
-60.161823	-1.911623	1.201152
-60.150831	-1.465607	1.206157
-60.145577	-4.150514	1.211162
-60.466435	2.768717	1.216166
-61.537008	4.993230	1.221171
-61.560572	2.187393	1.226176
-61.601023	8.349791	1.231181
-61.456488	4.286927	1.236186
-61.756131	-1.119625	1.241190
-62.806094	6.002441	1.246195
-62.878746	0.232500	1.251200
-63.180857	7.517445	1.256205
-62.711212	-1.125883	1.261210
-63.018017	1.765820	1.266214
-63.371849	-4.304663	1.271219
-63.828084	-1.271393	1.276224
-64.468432	2.364240	1.281229
-64.738624	3.157163	1.286234
-64.964460	-0.297161	1.291238
-65.472342	-1.456164	1.296243
-64.822054	-1.615074	1.301248
-65.038068	-3.013825	1.306253
-65.113057	-0.765929	1.311258
-65.276870	-6.153139	1.316262
-66.130868	-6.690451	1.321267
-66.301279	-0.800561	1.326272
-66.584830	0.103897	1.331277
-66.936620	-2.019670	1.336282
-67.150158	-8.123448	1.341286
-67.722511	4.041698	1.346291
-67.778594	-2.221753	1.351296
-67.994095	4.877365	1.356301
-68.121564	0.035879	1.361306
-67.871546	2.003019	1.366310
-68.580611	-11.024219	1.371315
-69.148119	-6.511468	1.376320
-69.683459	-1.521762	1.381325
-69.700816	-0.307372	1.386330
-69.972467	-1.764989	1.391334
-69.980235	-0.059446	1.396339
-69.931334	-0.167307	1.401344
-70.033823	-2.589284	1.406349
-69.942817	-5.773042	1.411354
-70.632059	-3.760073	1.416358
-71.083714	-6.678337	1.421363
-71.089260	-7.699713	1.426368
-71.511586	-3.920417	1.431373
-71.990246	-5.224167	1.436378
-72.505030	-12.832250	1.441382
-73.083865	-8.395176	1.446387
-72.897313	-10.943359	1.451392
-73.089597	-1.942247	1.456397
-73.100160	3.040672	1.461402
-73.026889	-2.355411	1.466406
-73.428475	-3.788550	1.471411
-72.941012	-5.277358	1.476416
-73.988604	-3.240169	1.481421
-74.421919	-7.407430	1.486426
-74.637479	-0.846037	1.491430
-74.747132	6.952266	1.496435
-75.467838	-10.122122	1.501440
-76.142442	-1.813693	1.506445
-76.338760	-1.394716	1.511450
-75.794542	-8.038382	1.516454
-76.422282	3.725878	1.521459
-76.358075	-10.627624	1.526464
-76.398284	-7.063753	1.531469
-76.577132	-12.343685	1.536474
-76.582914	-11.728145	1.541478
-77.423850	0.625333	1.546483
-77.634008	0.924256	1.551488
-77.858493	0.243227	1.556493
-77.878645	-3.572532	1.561498
-78.268583	3.566919	1.566502
-78.939124	-0.015234	1.571507
-79.281166	-2.808189	1.576512
-79.326933	5.342429	1.581517
-79.519673	-1.890975	1.586522
-79.414517	-0.637674	1.591526
-79.576164	2.858892	1.596531
-79.800918	-3.482197	1.601536
-81.075202	5.599440	1.606541
-81.392388	6.695357	1.611546
-80.936845	5.282084	1.616550
-81.212232	-0.712589	1.621555
-81.027442	-5.717081	1.626560
-81.277481	2.607273	1.631565
-81.380294	4.203053	1.636570
-81.848729	-2.326193	1.641574
-82.378204	1.826839	1.646579
-82.731585	-4.864920	1.651584
-82.456385	4.930593	1.656589
-83.110562	-2.329795	1.661594
-83.910371	-1.114288	1.666598
-84.099523	2.841094	1.671603
-83.802158	-7.529373	1.676608
-84.087358	-6.317987	1.681613
-84.440898	-4.775208	1.686618
-84.098399	-10.034526	1.691622
-85.101802	2.484191	1.696627
-85.170475	-6.103137	1.701632
-85.707955	-2.906832	1.706637
-85.673657	-6.779362	1.711642
-85.674839	-3.866838	1.716646
-85.792170	4.709833	1.721651
-86.286561	-1.137669	1.726656
-86.924742	1.579613	1.731661
-87.449215	-1.823080	1.736666
-87.089555	-2.735626	1.741670
-87.263927	3.755011	1.746675
-87.332597	-0.362527	1.751680
-88.257453	-2.014871	1.756685
-88.442148	-12.155134	1.761690
-88.810273	7.025715	1.766694
-89.067390	1.808470	1.771699
-88.842737	-1.297572	1.776704
-89.190755	-0.118010	1.781709
-89.384337	-1.265718	1.786714
-89.241191	-3.898869	1.791718
-89.569679	3.160549	1.796723
-90.153571	3.204844	1.801728
-90.683151	-1.071188	1.806733
-90.632213	1.158024	1.811738
-90.643739	-1.028404	1.816742
-90.959020	-0.554796	1.821747
-91.312805	-10.762368	1.826752
-92.045196	-2.993546	1.831757
-92.247449	2.292057	1.836762
-92.459025	-6.414276	1.841766
-92.678339	-8.510642	1.846771
-92.322171	-7.983856	1.851776
-92.391577	-2.674672	1.856781
-92.999667	-5.894203	1.861786
-93.454421	-3.704775	1.866790
-93.686700	6.497422	1.871795
-93.639919	0.963645	1.876800
-94.122766	9.933161	1.881805
-94.625218	5.152789	1.886810
-94.685506	-7.825403	1.891814
-95.565315	2.212499	1.896819
-95.436202	3.898530	1.901824
-95.237331	7.571007	1.906829
-95.313987	5.653871	1.911834
-95.541236	1.847940	1.916838
-96.453593	2.733993	1.921843
-96.790562	-2.258880	1.926848
-97.052591	9.568941	1.931853
-97.381710	3.866340	1.936858
-96.998672	-4.061125	1.941862
-97.373615	10.140764	1.946867
-97.201171	3.365472	1.951872
-97.981969	7.511980	1.956877
-98.383061	2.543144	1.961882
-98.400115	6.498243	1.966886
-98.909448	8.009796	1.971891
-98.695143	7.782584	1.976896
-98.906725	-3.458295	1.981901
-99.385798	10.997442	1.986906
-99.849013	-7.197418	1.991910
-100.471450	-2.376015	1.996915
-100.406074	-2.500686	2.006912
-99.297702	-1.584309	2.016909
-99.431386	1.653714	2.026906
-99.094223	2.690502	2.036902
-98.766876	6.443745	2.046899
-97.741454	0.605757	2.056896
-97.352680	-3.285689	2.066893
-96.982620	-0.257943	2.076890
-95.928082	3.235570	2.086886
-95.707834	3.542081	2.096883
-95.877536	-0.080432	2.106880
-95.065769	-2.110134	2.116877
-94.603587	0.520225	2.126874
-94.037982	3.221975	2.136870
-93.330732	1.833557	2.146867
-93.127571	-2.358895	2.156864
-92.219143	-3.330332	2.166861
-91.622901	0.633857	2.176858
-91.307897	6.793763	2.186854
-91.034713	3.050878	2.196851
-90.113106	1.964042	2.206848
-89.778266	-2.090569	2.216845
-89.864525	-1.931476	2.226842
-88.894794	-1.374662	2.236838
-88.333029	-2.425614	2.246835
-88.006276	7.378595	2.256832
-87.202145	7.377191	2.266829
-86.891614	0.488877	2.276826
-86.583600	-0.344002	2.286822
-85.607733	5.662596	2.296819
-85.054726	-4.818859	2.306816
-85.187036	1.118351	2.316813
-84.224066	1.720545	2.326810
-83.748135	-0.437490	2.336806
-83.815584	-2.547228	2.346803
-82.770780	2.380990	2.356800
-82.072493	2.164556	2.366797
-81.878970	-1.484520	2.376794
-81.387233	-3.263438	2.386790
-80.663806	1.953723	2.396787
-80.307359	-3.452988	2.406784
-80.282481	-5.949674	2.416781
-79.538642	-3.495575	2.426778
-78.911346	1.162532	2.436774
-77.940383	-4.533061	2.446771
-77.615132	-1.702196	2.456768
-77.717156	-2.943549	2.466765
-76.961665	-0.209027	2.476762
-76.045717	2.276045	2.486758
-75.757783	4.698754	2.496755
-75.656685	2.867953	2.506752
-74.430229	-0.817233	2.516749
-74.391268	2.547501	2.526746
-74.307400	-0.052808	2.536742
-73.194061	4.476202	2.546739
-72.684026	-7.070433	2.556736
-72.515246	0.227678	2.566733
-71.778533	0.731998	2.576730
-71.337507	5.753887	2.586726
-71.113246	3.548814	2.596723
-70.379994	-0.613269	2.606720
-69.497376	-0.054077	2.616717
-69.648127	0.207573	2.626714
-69.033232	-2.528493	2.636710
-68.434264	-3.849775	2.646707
-67.445845	-0.384427	2.656704
-66.895393	-3.704356	2.666701
-66.785631	1.506157	2.676698
-66.868568	1.091700	2.686694
-65.967916	0.595367	2.696691
-65.501410	-3.524713	2.706688
-64.583977	-4.797176	2.716685
-63.814388	0.985738	2.726682
-63.811815	-1.311250	2.736678
-63.609705	2.540782	2.746675
-63.084026	-6.107885	2.756672
-62.561515	-1.952469	2.766669
-61.601276	-4.057730	2.776666
-60.885782	1.787689	2.786662
-60.797461	-4.989729	2.796659
-60.589489	-2.974437	2.806656
-60.079380	-4.017622	2.816653
-59.086479	-4.069448	2.826650
-58.975442	3.377131	2.836646
-58.024154	-10.574878	2.846643
-57.357624	-4.120692	2.856640
-57.210111	-8.098241	2.866637
-57.560038	-3.679400	2.876634
-56.602759	0.343163	2.886630
-55.776198	3.063549	2.896627
-54.867623	1.211060	2.906624
-54.446974	5.494194	2.916621
-54.508365	5.067871	2.926618
-54.158343	4.676952	2.936614
-53.072586	3.514334	2.946611
-53.034022	7.488688	2.956608
-52.144078	1.565064	2.966605
-51.244905	-2.332659	2.976602
-51.280512	5.855443	2.986598
-50.941331	1.419761	2.996595
-50.583496	1.362258	3.006592
-49.754878	2.610488	3.016589
-49.583585	-0.263334	3.026586
-48.338185	-3.245479	3.036582
-48.157910	-3.406157	3.046579
-47.950026	-4.754748	3.056576
-47.312943	-6.428905	3.066573
-46.393922	-3.877354	3.076570
-46.431261	-5.867995	3.086566
-46.126151	-7.311326	3.096563
-45.092263	-7.894724	3.106560
-45.019574	-1.215739	3.116557
-43.912764	-1.545064	3.126554
-43.726391	-9.657603	3.136550
-43.605728	-7.819907	3.146547
-42.926269	-4.226924	3.156544
-42.225022	-3.557866	3.166541
-41.870886	0.736678	3.176538
-41.151644	-3.130456	3.186534
-40.742968	2.382658	3.196531
-40.589133	-3.790723	3.206528
-39.348516	-5.186447	3.216525
-38.946061	2.077319	3.226522
-38.731848	2.358356	3.236518
-38.718284	0.370744	3.246515
-37.456114	1.863714	3.256512
-37.285670	-2.906792	3.266509
-36.862257	-2.105182	3.276506
-36.145929	-1.206458	3.286502
-35.691062	5.711155	3.296499
-35.524687	-4.734529	3.306496
-34.436882	-2.418192	3.316493
-34.185784	1.834930	3.326490
-34.134684	2.503375	3.336486
-33.165900	2.096733	3.346483
-32.438489	-3.210376	3.356480
-32.289615	0.064040	3.366477
-32.005811	0.214408	3.376474
-31.332363	-0.777182	3.386470
-30.792481	1.531097	3.396467
-29.442156	2.050784	3.406464
-29.899740	0.829187	3.416461
-29.647820	-1.595438	3.426458
-28.554078	-7.577304	3.436454
-27.969534	-2.190921	3.446451
-27.704195	-8.938771	3.456448
-27.557870	-3.076351	3.466445
-26.423144	-0.720953	3.476442
-26.157477	2.600116	3.486438
-26.188454	0.244467	3.496435
-25.250845	3.292048	3.506432
-24.393712	-1.990108	3.516429
-24.589425	2.641485	3.526426
-23.471636	2.842446	3.536422
-22.792406	5.305084	3.546419
-22.618526	6.551883	3.556416
-22.615016	-1.965267	3.566413
-21.879361	2.709090	3.576410
-21.327759	3.309474	3.586406
-20.423474	5.994868	3.596403
-19.701817	3.406112	3.606400
-19.563278	5.232355	3.616397
-19.503940	1.428857	3.626394
-18.890675	3.836623	3.636390
-18.089726	7.390923	3.646387
-18.008183	2.912349	3.656384
-17.023681	11.157967	3.666381
-16.602948	6.812710	3.676378
-16.283480	4.020849	3.686374
-15.624886	4.663188	3.696371
-15.028952	3.742723	3.706368
-14.959450	9.348561	3.716365
-14.217355	3.676648	3.726362
-13.679305	10.442380	3.736358
-13.599660	5.322558	3.746355
-11.979172	-3.490210	3.756352
-11.744903	-1.056633	3.766349
-11.486445	-4.704804	3.776346
-11.694047	1.753068	3.786342
-11.143918	5.275796	3.796339
-10.396363	4.799689	3.806336
-9.483903	-2.892692	3.816333
-8.700508	-0.042052	3.826330
-8.652733	-2.486615	3.836326
-8.464433	0.302918	3.846323
-7.686640	-3.876608	3.856320
-7.039142	0.504116	3.866317
-6.868128	-5.405369	3.876314
-6.192043	-5.120198	3.886310
-5.620648	-0.821515	3.896307
-5.274751	-7.295021	3.906304
-4.427025	-5.854930	3.916301
-4.121773	3.003847	3.926298
-3.831898	3.950670	3.936294
-3.555145	13.735713	3.946291
-2.972197	21.511783	3.956288
-2.533767	32.499843	3.966285
-2.227452	51.756852	3.976282
-1.534273	62.502990	3.986278
-1.290894	75.963774	3.996275
-0.675817	97.333290	4.006272
-0.383724	115.416300	4.016269
0.000000	143.335442	4.021274
0.402837	149.855872	4.026278
0.301399	160.162605	4.031283
0.668163	154.201241	4.036288
0.875985	162.388101	4.041293
0.554752	168.743879	4.046298
0.978942	164.972897	4.051302
0.825802	169.533111	4.056307
1.034370	169.235811	4.061312
1.063745	177.003881	4.066317
0.971924	181.370620	4.071322
1.125143	170.622914	4.076326
1.358744	196.978944	4.081331
1.336404	187.190341	4.086336
1.336517	184.623863	4.091341
0.974646	174.861692	4.096346
1.098460	171.579716	4.101350
0.818923	185.415111	4.106355
1.246450	192.253916	4.111360
1.359312	194.376802	4.116365
1.176855	205.310301	4.121370
1.628902	198.019753	4.126374
1.213738	202.183502	4.131379
1.218211	202.281714	4.136384
1.254465	194.192530	4.141389
1.129278	210.109539	4.146394
1.333795	197.407982	4.151398
1.013567	198.403966	4.156403
1.413002	202.728042	4.161408
1.410560	207.550831	4.166413
1.244863	205.237558	4.171418
1.538169	197.721494	4.176422
0.815979	212.131049	4.181427
1.384152	205.049586	4.186432
1.642848	206.493170	4.191437
1.191792	213.566467	4.196442
1.565761	200.846320	4.201446
1.463517	207.897967	4.206451
1.476467	212.097193	4.211456
1.442034	203.366921	4.216461
1.382965	209.262530	4.221466
1.461384	206.024769	4.226470
1.166041	213.114314	4.231475
1.484753	200.353786	4.236480
1.636883	217.152952	4.241485
1.263949	212.002952	4.246490
1.765468	213.839481	4.251494
1.439198	213.436960	4.256499
1.353259	215.606582	4.261504
1.556481	217.656097	4.266509
1.577227	235.619812	4.271514
1.750710	227.738967	4.276518
1.785208	241.172139	4.281523
1.851098	232.938904	4.286528
1.490766	222.442358	4.291533
1.594391	233.124459	4.296538
1.828043	232.868984	4.301542
1.652247	237.545845	4.306547
1.776301	233.901113	4.311552
1.648231	227.649484	4.316557
1.642832	242.066669	4.321562
2.013713	237.544950	4.326566
1.802929	249.833937	4.331571
1.852054	239.506382	4.336576
2.193518	234.477447	4.341581
1.491043	225.085409	4.346586
1.800774	225.614377	4.351590
1.537067	242.958206	4.356595
1.982829	234.001387	4.361600
1.749387	233.942448	4.366605
1.808095	237.869673	4.371610
1.744328	236.497387	4.376614
1.656751	236.032055	4.381619
1.950501	236.477236	4.386624
1.917067	239.978475	4.391629
1.662744	238.628271	4.396634
1.991968	228.165540	4.401638
1.936176	242.205080	4.406643
1.939373	234.645868	4.411648
2.342758	239.384298	4.416653
2.081046	238.997529	4.421658
2.231628	234.163597	4.426662
2.003091	237.542826	4.431667
1.870769	240.291617	4.436672
2.027060	242.155321	4.441677
1.977166	232.870117	4.446682
2.227198	231.456132	4.451686
2.176094	235.514810	4.456691
2.270290	238.106113	4.461696
2.233645	239.758448	4.466701
1.645542	246.664418	4.471706
2.298288	230.699854	4.476710
2.134258	249.200151	4.481715
2.223968	243.240624	4.486720
2.469154	236.381747	4.491725
2.321738	241.856674	4.496730
2.315750	237.984436	4.501734
1.960869	242.245763	4.506739
2.198313	235.605040	4.511744
2.201240	238.686444	4.516749
1.989557	242.426376	4.521754
2.520642	225.364842	4.526758
1.978966	237.377482	4.531763
2.034094	240.973184	4.536768
2.012126	240.851600	4.541773
1.845900	234.543929	4.546778
2.213537	237.175793	4.551782
2.018894	253.463500	4.556787
2.369692	262.426937	4.561792
2.454479	267.444083	4.566797
2.316106	273.285754	4.571802
2.543294	269.397195	4.576806
2.522558	274.121603	4.581811
2.469720	267.380143	4.586816
2.682229	267.510015	4.591821
2.159065	264.260559	4.596826
2.543472	263.543809	4.601830
2.684616	270.453554	4.606835
2.725165	263.209408	4.611840
2.600484	244.149872	4.616845
1.846641	247.364681	4.621850
2.268661	250.402541	4.626854
2.483938	265.521639	4.631859
2.676230	269.106475	4.636864
2.567760	268.645982	4.641869
2.442679	271.612032	4.646874
2.728253	262.706784	4.651878
2.456102	275.578230	4.656883
2.635312	268.932336	4.661888
2.543512	271.986412	4.666893
2.738817	270.048479	4.671898
2.569585	267.976138	4.676902
2.676852	276.018485	4.681907
2.737893	264.901763	4.686912
2.671222	276.560690	4.691917
2.769585	277.953474	4.696922
2.852561	271.007382	4.701926
2.750915	274.595306	4.706931
2.538912	275.301444	4.711936
2.979048	269.756897	4.716941
2.668089	272.049826	4.721946
2.606772	275.278630	4.726950
2.278011	279.606682	4.731955
2.747995	277.753704	4.736960
2.899099	274.049032	4.741965
2.248681	278.494086	4.746970
2.630275	277.244992	4.751974
2.603775	280.152292	4.756979
3.051904	267.293911	4.761984
2.677275	268.224314	4.766989
2.602930	273.926324	4.771994
2.968386	274.110594	4.776998
3.085654	285.545088	4.782003
2.932440	285.738283	4.787008
2.796538	282.080739	4.792013
2.931614	289.551934	4.797018
2.973862	286.127545	4.802022
2.868458	295.408083	4.807027
3.152155	288.707583	4.812032
3.175083	292.815784	4.817037
2.723810	289.980864	4.822042
3.164610	291.424495	4.827046
3.006127	295.762639	4.832051
3.153402	296.580969	4.837056
2.818138	289.340234	4.842061
2.738518	291.525199	4.847066
3.411125	301.744702	4.852070
3.161791	304.021314	4.857075
3.039102	301.765237	4.862080
3.519970	301.008240	4.867085
2.540780	302.599585	4.872090
2.982857	295.074233	4.877094
3.000667	308.535288	4.882099
2.827903	299.664078	4.887104
2.960247	301.364215	4.892109
2.978566	309.897680	4.897114
2.926902	290.826785	4.902118
3.019845	305.865736	4.907123
2.748523	301.175449	4.912128
3.164543	313.948761	4.917133
3.295560	339.718564	4.922138
3.562362	331.122653	4.927142
3.482032	319.356182	4.932147
3.386480	311.791183	4.937152
3.342117	310.750953	4.942157
3.255668	305.377458	4.947162
3.522973	300.815052	4.952166
3.281697	300.793918	4.957171
3.139761	300.843557	4.962176
3.229878	300.663354	4.967181
3.387568	320.868342	4.972186
3.603726	317.390087	4.977190
3.579670	307.642541	4.982195
3.311619	314.299785	4.987200
3.538293	304.477767	4.992205
3.467036	314.132734	4.997210
3.680035	307.128390	5.002214
3.325547	307.912983	5.007219
3.265130	313.293015	5.012224
3.530770	300.702023	5.017229
3.600245	317.729096	5.022234
3.749623	308.328955	5.027238
3.370592	309.532415	5.032243
3.264606	308.822668	5.037248
3.714084	313.426009	5.042253
3.662898	330.077611	5.047258
3.999750	310.299828	5.052262
3.295619	315.554976	5.057267
3.337967	305.905760	5.062272
3.916516	320.203827	5.067277
3.426211	315.758185	5.072282
3.437101	322.120598	5.077286
3.218655	328.112106	5.082291
3.639948	335.774708	5.087296
3.903468	331.192594	5.092301
3.518059	336.303408	5.097306
3.772165	325.523497	5.102310
3.780633	340.670402	5.107315
3.829942	330.064706	5.112320
4.061086	334.893651	5.117325
3.966285	336.420450	5.122330
3.812845	328.641642	5.127334
4.200759	340.520955	5.132339
4.132014	328.785910	5.137344
3.990441	322.209687	5.142349
3.418434	313.989092	5.147354
3.688270	302.395339	5.152358
3.684415	300.404736	5.157363
3.825387	316.209108	5.162368
3.910035	322.077015	5.167373
3.953106	327.957335	5.172378
4.342580	325.324781	5.177382
3.725908	314.440620	5.182387
3.882458	300.566253	5.187392
3.751481	302.874377	5.192397
3.642991	312.352774	5.197402
3.754716	321.636053	5.202406
4.117330	338.917916	5.207411
3.968591	335.846604	5.212416
4.101258	337.378165	5.217421
3.535966	341.362171	5.222426
3.686269	336.953713	5.227430
3.589735	341.427050	5.232435
3.554794	344.015086	5.237440
4.086166	339.314615	5.242445
3.972132	344.404373	5.247450
4.244760	343.288168	5.252454
3.874511	351.006662	5.257459
3.692615	348.616917	5.262464
4.355022	350.956081	5.267469
4.128568	370.678119	5.272474
4.177604	367.200688	5.277478
4.139868	367.628736	5.282483
4.083069	363.051503	5.287488
4.081966	361.688366	5.292493
4.066267	372.846962	5.297498
4.207921	369.715125	5.302502
4.261441	369.994070	5.307507
4.479018	370.440818	5.312512
4.239203	369.802562	5.317517
4.389942	376.883042	5.322522
4.469528	366.763286	5.327526
4.381140	367.204851	5.332531
3.904166	348.315019	5.337536
4.363654	355.657341	5.342541
4.142645	369.047880	5.347546
4.665180	364.950746	5.352550
4.395126	366.007500	5.357555
4.374847	365.883860	5.362560
4.455345	373.244744	5.367565
4.297697	376.955632	5.372570
4.238713	372.811126	5.377574
3.958522	372.603833	5.382579
3.905587	378.157491	5.387584
4.055797	369.732815	5.392589
3.893019	389.530767	5.397594
4.549497	372.401342	5.402598
4.171462	368.255992	5.407603
4.360836	371.789632	5.412608
4.388672	381.889412	5.417613
4.645254	398.692199	5.422618
4.667346	394.155176	5.427622
4.528362	401.241016	5.432627
4.359850	406.386190	5.437632
4.506232	399.606355	5.442637
4.541212	405.916466	5.447642
4.692369	408.207686	5.452646
4.866372	406.577756	5.457651
4.763839	395.520192	5.462656
5.029761	381.866224	5.467661
4.782710	385.475489	5.472666
4.575421	372.641878	5.477670
4.676170	380.332518	5.482675
4.363891	374.390369	5.487680
4.628685	372.674762	5.492685
4.359332	382.900912	5.497690
4.992583	388.177159	5.502694
4.854725	389.398706	5.507699
4.773417	381.991158	5.512704
4.908368	373.667478	5.517709
4.661839	374.249094	5.522714
4.712897	370.266932	5.527718
4.575377	379.608488	5.532723
4.791231	386.823826	5.537728
5.057592	394.884489	5.542733
4.709990	389.067770	5.547738
5.053903	383.853279	5.552742
4.796851	384.392039	5.557747
4.813521	389.669742	5.562752
4.802321	383.462438	5.567757
5.212284	401.583112	5.572762
5.067390	384.051979	5.577766
4.816262	377.853424	5.582771
4.577776	370.085323	5.587776
5.033528	386.607853	5.592781
4.849544	409.440852	5.597786
5.147455	399.752021	5.602790
4.703072	394.782515	5.607795
4.966562	394.084203	5.612800
5.233984	399.898589	5.617805
4.857520	406.480089	5.622810
5.286124	395.077049	5.627814
4.878350	401.139600	5.632819
4.776786	397.886017	5.637824
4.871186	401.448612	5.642829
4.943278	410.675754	5.647834
5.089683	408.977773	5.652838
5.057090	400.974278	5.657843
5.154281	401.907272	5.662848
5.076402	397.615911	5.667853
4.846046	403.425896	5.672858
5.236669	404.810357	5.677862
5.315093	399.649097	5.682867
4.807581	407.201100	5.687872
5.138586	403.641252	5.692877
4.796971	397.705135	5.697882
5.064162	402.908798	5.702886
5.043260	404.687209	5.707891
4.935224	406.764215	5.712896
5.208934	403.691019	5.717901
4.890131	421.378461	5.722906
5.422371	430.716497	5.727910
5.262720	431.067446	5.732915
5.243273	429.681883	5.737920
5.314471	426.517103	5.742925
5.207640	436.358799	5.747930
5.568621	423.188716	5.752934
5.193521	422.906362	5.757939
5.341050	436.449849	5.762944
5.367125	429.716761	5.767949
5.651838	426.278437	5.772954
5.546165	434.365599	5.777958
5.395731	440.892715	5.782963
5.409329	435.478335	5.787968
5.575647	433.663388	5.792973
5.515475	438.672032	5.797978
5.562631	437.723399	5.802982
5.650202	430.851068	5.807987
5.324059	426.089306	5.812992
5.632064	425.726992	5.817997
5.543734	431.514653	5.823002
5.365082	419.091857	5.828006
5.212962	424.977303	5.833011
5.291421	431.591427	5.838016
5.255918	424.799864	5.843021
5.312186	433.064850	5.848026
5.376735	436.137274	5.853030
5.233289	440.070791	5.858035
4.951211	437.923179	5.863040
5.513530	443.889247	5.868045
5.693424	460.190140	5.873050
5.822025	462.449384	5.878054
5.737032	462.862960	5.883059
5.736823	459.823665	5.888064
5.561591	440.620899	5.893069
5.407076	452.052764	5.898074
5.769157	458.638486	5.903078
5.807446	464.730210	5.908083
5.562406	462.414446	5.913088
5.882797	459.911713	5.918093
5.326230	469.851187	5.923098
5.588266	463.044873	5.928102
5.630337	462.767244	5.933107
5.533412	471.987480	5.938112
5.733697	469.223030	5.943117
5.672523	472.231818	5.948122
5.852099	470.790997	5.953126
5.906153	468.023134	5.958131
5.830702	474.121263	5.963136
5.993576	464.096583	5.968141
5.885373	469.621338	5.973146
5.894969	461.318961	5.978150
5.948933	470.197876	5.983155
5.957362	465.901677	5.988160
6.343794	465.967230	5.993165
5.932679	460.463720	5.998170
6.176508	467.177958	6.003174
5.551135	465.308602	6.008179
5.680446	479.281198	6.013184
6.039944	466.441867	6.018189
5.902676	468.686724	6.023194
5.813415	467.572417	6.028198
6.158851	460.373995	6.033203
5.740555	472.463673	6.038208
6.171189	464.384427	6.043213
5.711850	474.398580	6.048218
5.866932	462.431201	6.053222
5.685327	471.746565	6.058227
6.096784	494.641528	6.063232
6.461703	489.256377	6.068237
6.065053	487.091814	6.073242
6.073022	479.656016	6.078246
6.131050	469.588505	6.083251
5.815947	470.797967	6.088256
6.413222	470.485238	6.093261
6.239705	464.986191	6.098266
6.187903	458.272301	6.103270
6.247166	464.877384	6.108275
6.207396	470.305952	6.113280
6.650454	460.028067	6.118285
6.202875	466.288852	6.123290
6.378924	468.595495	6.128294
6.569794	457.077653	6.133299
6.254331	451.158103	6.138304
6.253435	445.003731	6.143309
5.814813	448.886275	6.148314
6.081769	432.389029	6.153318
5.794333	432.601884	6.158323
5.482003	435.685603	6.163328
5.937737	428.900117	6.168333
5.714248	443.168301	6.173338
5.901326	448.265066	6.178342
6.158117	466.991554	6.183347
5.692237	474.127611	6.188352
6.131935	466.061071	6.193357
5.898818	482.127461	6.198362
6.295940	473.349258	6.203366
5.990275	472.089035	6.208371
5.711273	472.952307	6.213376
5.987828	465.889216	6.218381
5.807897	477.463446	6.223386
5.772630	476.708828	6.228390
5.923458	473.426460	6.233395
6.021379	472.294182	6.238400
6.148155	464.209601	6.243405
6.524488	466.788758	6.248410
6.092699	462.554009	6.253414
6.053683	470.356837	6.258419
6.088529	464.081095	6.263424
6.137496	467.742005	6.268429
6.148706	464.668060	6.273434
6.201042	461.945673	6.278438
5.871636	445.501577	6.283443
5.883795	462.090340	6.288448
6.254454	456.319439	6.293453
5.974354	451.172930	6.298458
6.084848	438.343872	6.303462
6.106166	438.497906	6.308467
5.821711	434.835323	6.313472
6.184815	437.634133	6.318477
5.755522	444.326421	6.323482
6.076055	440.649500	6.328486
6.068409	452.395680	6.333491
5.911334	452.999191	6.338496
6.097962	453.982698	6.343501
6.124444	458.461944	6.348506
5.803218	439.215075	6.353510
6.053421	454.174651	6.358515
5.914745	467.505069	6.363520
6.004925	471.707956	6.368525
6.219141	476.931467	6.373530
6.064544	458.112837	6.378534
5.813671	453.124688	6.383539
5.862318	473.257156	6.388544
5.971915	465.624563	6.393549
5.915177	468.626103	6.398554
6.194361	473.886217	6.403558
6.061473	469.814506	6.408563
6.053480	469.618183	6.413568
6.188583	474.175355	6.418573
6.235516	459.177192	6.423578
5.920162	441.264742	6.428582
5.700128	448.059333	6.433587
5.759677	463.822676	6.438592
6.323904	452.834439	6.443597
6.213409	470.144469	6.448602
5.948124	454.380829	6.453606
5.949057	446.095878	6.458611
5.971798	449.848943	6.463616
6.060003	448.729721	6.468621
6.025346	465.593831	6.473626
6.045492	458.571229	6.478630
5.960914	459.634377	6.483635
5.906574	456.445977	6.488640
6.394019	455.646443	6.493645
6.058666	447.253188	6.498650
6.063159	448.600554	6.503654
5.653650	437.147609	6.508659
5.695903	448.104060	6.513664
6.307582	450.903350	6.518669
6.314647	462.101655	6.523674
5.969224	441.789014	6.528678
6.019553	441.788859	6.533683
5.829424	445.474752	6.538688
6.057979	443.679888	6.543693
5.926788	455.260633	6.548698
6.010953	453.229781	6.553702
6.290808	461.949726	6.558707
6.011256	450.217526	6.563712
5.969692	436.623503	6.568717
5.761646	430.689332	6.573722
5.911170	453.680296	6.578726
6.031752	457.538130	6.583731
6.198080	474.572229	6.588736
6.117406	455.013574	6.593741
6.049661	446.557260	6.598746
6.016066	434.635945	6.603750
5.858173	440.954327	6.608755
5.901079	452.520648	6.613760
6.271062	452.250292	6.618765
5.969126	451.094832	6.623770
5.752015	436.196064	6.628774
5.827797	450.063238	6.633779
6.028310	464.857591	6.638784
6.313227	468.465617	6.643789
6.115675	469.970370	6.648794
6.261161	441.212219	6.653798
6.329419	431.949759	6.658803
5.629969	438.730194	6.663808
6.030835	430.352782	6.668813
5.879439	441.535081	6.673818
5.899248	429.588943	6.678822
5.952338	444.267775	6.683827
5.888815	460.746521	6.688832
6.424555	444.963325	6.693837
6.066979	454.893915	6.698842
6.071173	432.076982	6.703846
6.265402	433.692489	6.708851
6.082603	440.979587	6.713856
6.452649	431.342336	6.718861
6.013235	442.499313	6.723866
6.266809	440.842785	6.728870
6.186123	425.456703	6.733875
5.967477	438.140833	6.738880
6.071966	426.417087	6.743885
6.077861	426.600316	6.748890
6.036014	435.814962	6.753894
6.049590	432.672747	6.758899
6.246668	432.210002	6.763904
6.503237	433.050104	6.768909
6.144932	432.574142	6.773914
5.984079	437.943222	6.778918
6.235344	436.588413	6.783923
6.270555	426.242118	6.788928
6.024207	415.356556	6.793933
5.891876	412.679556	6.798938
5.706852	405.753705	6.803942
5.966107	409.236118	6.808947
5.903543	436.732683	6.813952
6.354429	429.939710	6.818957
6.237139	430.370276	6.823962
6.107347	412.016077	6.828966
5.978303	410.433170	6.833971
5.441342	425.515169	6.838976
5.962726	425.725719	6.843981
5.692681	438.596360	6.848986
5.976861	433.728403	6.853990
6.049515	444.662057	6.858995
5.739736	446.758464	6.864000
5.875422	439.241744	6.869005
6.078859	449.604749	6.874010
6.185818	444.050978	6.879014
6.150739	439.813496	6.884019
5.849555	429.844959	6.889024
6.350270	435.158167	6.894029
6.217769	441.050828	6.899034
6.147041	433.596312	6.904038
5.998340	440.696015	6.909043
5.657120	443.110607	6.914048
5.780105	444.286796	6.919053
5.627326	445.096407	6.924058
5.748226	440.799154	6.929062
5.806779	441.445698	6.934067
5.691981	443.856345	6.939072
5.698388	444.860418	6.944077
5.947965	447.980352	6.949082
6.087919	439.433013	6.954086
6.140760	433.707050	6.959091
6.040722	438.371624	6.964096
6.140080	424.512142	6.969101
5.985298	431.871756	6.974106
6.002230	437.392948	6.979110
6.001325	430.933102	6.984115
6.469542	443.921464	6.989120
6.608133	442.234049	6.994125
5.878785	448.593778	6.999130
6.150035	441.577360	7.004134
6.185939	439.772561	7.009139
5.734275	438.477512	7.014144
6.031450	435.980995	7.019149
5.884393	442.506960	7.024154
5.895559	440.458597	7.029158
6.117604	441.491888	7.034163
5.754327	448.231460	7.039168
6.129377	445.399990	7.044173
5.839972	451.155042	7.049178
5.700185	443.148949	7.054182
6.049174	444.313960	7.059187
5.898108	452.758530	7.064192
6.143237	440.557606	7.069197
5.658096	448.741159	7.074202
5.923515	443.844139	7.079206
6.161398	446.457861	7.084211
6.105754	447.803147	7.089216
6.238079	447.617138	7.094221
5.778708	450.324609	7.099226
6.105649	444.931949	7.104230
5.785866	445.559442	7.109235
5.980498	446.883414	7.114240
5.795547	431.215426	7.119245
6.162169	440.193713	7.124250
5.898753	442.380519	7.129254
5.916949	442.467580	7.134259
5.907795	444.990781	7.139264
6.154937	442.846904	7.144269
6.016347	448.694004	7.149274
6.169724	442.827856	7.154278
5.883827	448.383607	7.159283
5.691863	448.136247	7.164288
6.076537	455.341028	7.169293
6.354569	475.135165	7.174298
6.503862	450.520099	7.179302
6.256365	443.291990	7.184307
6.303316	443.293776	7.189312
6.278987	437.156706	7.194317
5.979813	439.489741	7.199322
6.275020	446.049431	7.204326
6.032253	442.206285	7.209331
6.015101	437.984188	7.214336
6.122087	435.266570	7.219341
5.947658	442.979916	7.224346
6.080688	446.202228	7.229350
6.269601	439.566890	7.234355
6.256774	446.695010	7.239360
6.275712	442.141720	7.244365
6.037060	439.098892	7.249370
5.931058	435.534833	7.254374
5.928409	429.799510	7.259379
5.959897	439.801237	7.264384
5.660561	434.387565	7.269389
5.857166	445.831537	7.274394
6.087290	431.426856	7.279398
6.275155	442.685393	7.284403
6.420901	440.388989	7.289408
6.408705	435.370599	7.294413
5.908596	416.355454	7.299418
5.967413	415.643869	7.304422
5.928489	411.158187	7.309427
5.980521	411.134464	7.314432
6.177613	406.813948	7.319437
5.894348	413.816333	7.324442
5.781669	413.655896	7.329446
6.031132	418.546956	7.334451
5.873460	426.129643	7.339456
5.892802	435.671804	7.344461
6.093673	448.644842	7.349466
6.113934	439.210353	7.354470
6.061747	446.506413	7.359475
5.843120	448.931886	7.364480
6.398030	434.794886	7.369485
6.306068	423.385867	7.374490
5.948534	420.784046	7.379494
5.938817	407.534657	7.384499
5.901319	415.274255	7.389504
5.864136	413.266660	7.394509
5.783013	421.563862	7.399514
5.767651	433.810572	7.404518
6.297960	440.961827	7.409523
5.977240	445.246758	7.414528
6.133463	440.183901	7.419533
5.850047	433.987908	7.424538
6.048538	441.295541	7.429542
6.046304	439.727746	7.434547
6.134608	441.656408	7.439552
6.272752	433.293686	7.444557
5.783586	421.997210	7.449562
5.949616	422.857829	7.454566
5.958291	430.337590	7.459571
5.620256	437.838653	7.464576
6.093486	432.678511	7.469581
6.031817	436.118756	7.474586
5.885961	431.553289	7.479590
6.208172	437.802630	7.484595
5.884714	437.603684	7.489600
5.865740	437.100937	7.494605
5.987584	441.283969	7.499610
6.022487	440.037213	7.504614
5.988873	435.819815	7.509619
5.833530	441.791446	7.514624
6.211922	432.297264	7.519629
6.037639	440.429140	7.524634
5.752128	441.564040	7.529638
6.122679	432.758685	7.534643
5.789703	442.825501	7.539648
6.124918	433.846615	7.544653
5.620471	433.875965	7.549658
5.722833	439.443002	7.554662
5.889220	436.245290	7.559667
5.834657	438.189714	7.564672
5.999023	439.652098	7.569677
6.004697	443.366546	7.574682
6.101938	439.427829	7.579686
5.874052	444.370707	7.584691
5.657779	448.025409	7.589696
6.181297	436.371394	7.594701
5.865592	440.731468	7.599706
5.751892	438.280490	7.604710
6.010410	436.804893	7.609715
5.791221	451.911458	7.614720
6.614594	457.517574	7.619725
6.194811	456.193959	7.624730
6.088928	439.021776	7.629734
6.129319	444.486002	7.634739
5.902679	446.902736	7.639744
5.889888	440.227387	7.644749
6.105424	452.083036	7.649754
6.113076	444.807547	7.654758
6.361963	440.981067	7.659763
5.736206	456.958720	7.664768
5.925919	446.554071	7.669773
5.959508	449.855998	7.674778
5.824938	446.735153	7.679782
6.013782	447.556475	7.684787
5.972506	444.396107	7.689792
6.127245	434.229327	7.694797
6.084791	442.764246	7.699802
5.980167	439.989313	7.704806
6.132560	436.892784	7.709811
5.915400	433.898496	7.714816
6.101447	438.958329	7.719821
6.117287	445.494816	7.724826
5.650020	450.575214	7.729830
5.911109	445.204509	7.734835
5.745830	440.654688	7.739840
6.000289	441.812856	7.744845
6.170581	449.003404	7.749850
6.097987	446.295984	7.754854
6.127261	437.912609	7.759859
6.044693	448.078074	7.764864
5.886901	436.659423	7.769869
5.916624	443.261297	7.774874
6.292992	441.949316	7.779878
6.019616	438.444544	7.784883
6.132312	448.176882	7.789888
6.475214	438.423349	7.794893
6.211936	446.155751	7.799898
5.980467	444.697548	7.804902
6.354490	439.904305	7.809907
6.098233	447.549899	7.814912
6.326061	442.059392	7.819917
6.292338	449.515398	7.824922
6.010225	449.977796	7.829926
6.274131	447.373908	7.834931
5.984597	455.561582	7.839936
6.060741	449.058580	7.844941
5.978882	453.034987	7.849946
5.844650	455.156200	7.854950
6.223869	440.572898	7.859955
6.094239	449.787682	7.864960
6.061953	442.597546	7.869965
6.113794	435.830390	7.874970
5.942606	430.322090	7.879974
5.941188	432.632263	7.884979
5.983918	436.791886	7.889984
5.799855	437.361780	7.894989
6.006825	437.578019	7.899994
5.759376	447.544438	7.904998
6.011504	446.159688	7.910003
5.971107	445.822700	7.915008
6.033927	445.120515	7.920013
6.016515	442.889609	7.925018
5.733607	453.507992	7.930022
5.916981	445.993436	7.935027
5.392714	448.878011	7.940032
5.842202	439.725683	7.945037
5.727964	445.123159	7.950042
5.747926	445.732284	7.955046
5.884398	439.582993	7.960051
5.835635	452.242160	7.965056
6.148216	443.348518	7.970061
5.877186	453.234385	7.975066
6.076410	454.635152	7.980070
6.127794	448.240051	7.985075
5.880603	446.946072	7.990080
5.917051	447.514381	7.995085
6.209024	461.532055	8.000090
6.112498	453.521950	8.005094
6.362498	440.654397	8.010099
5.831253	441.000572	8.015104
6.330647	435.845568	8.020109
5.978599	447.340437	8.025126
6.224256	441.717788	8.030144
6.270519	441.628332	8.035162
5.807131	447.412594	8.040179
5.925621	441.850960	8.045197
5.869389	438.242130	8.050214
5.876902	440.738028	8.055232
6.091860	438.258219	8.060250
5.864572	445.400523	8.065267
6.321350	441.034157	8.070285
6.002353	444.899180	8.075302
5.994639	434.748166	8.080320
6.030677	435.161545	8.085338
6.203047	444.909711	8.090355
6.212223	436.913413	8.095373
6.286237	441.336932	8.100390
5.764217	449.535249	8.105408
5.931042	451.100506	8.110426
5.850548	449.492785	8.115443
6.151253	450.395567	8.120461
5.939768	458.787332	8.125478
6.281054	470.276506	8.130496
6.515730	471.726207	8.135514
6.282216	459.599723	8.140531
5.921581	445.868240	8.145549
6.046898	441.442988	8.150566
5.962074	455.644243	8.155584
5.949959	452.799699	8.160602
5.977515	467.978541	8.165619
6.228949	466.678230	8.170637
6.198308	469.898704	8.175654
6.099505	474.666180	8.180672
6.425193	465.142172	8.185690
6.169542	481.135385	8.190707
6.580682	470.975025	8.195725
6.087616	459.220039	8.200742
6.090793	456.804624	8.205760
6.261845	462.172048	8.210778
6.052863	459.754758	8.215795
6.208359	464.774785	8.220813
6.286455	468.434110	8.225830
6.211805	477.104975	8.230848
6.432263	465.017480	8.235866
6.062862	458.509540	8.240883
6.260569	464.628794	8.245901
6.063708	459.472299	8.250918
6.078955	472.892685	8.255936
6.595946	466.588728	8.260954
6.226766	475.370760	8.265971
6.007847	474.297534	8.270989
6.220482	469.597402	8.276006
6.104844	481.056151	8.281024
6.592082	472.315368	8.286042
6.240602	482.024916	8.291059
6.036880	469.724211	8.296077
6.187603	476.873025	8.301094
5.812395	486.179251	8.306112
6.143602	474.988697	8.311130
6.086623	483.355874	8.316147
6.276578	484.638192	8.321165
6.348585	471.054715	8.326182
6.133096	477.540010	8.331200
6.288111	476.590678	8.336218
6.377856	475.036845	8.341235
6.317343	486.525837	8.346253
6.453522	488.284742	8.351270
6.279560	482.874662	8.356288
6.259559	475.076862	8.361306
6.148584	477.557153	8.366323
6.249754	477.827475	8.371341
6.396266	476.367975	8.376358
6.161129	476.268032	8.381376
6.367300	485.508105	8.386394
6.463508	496.805220	8.391411
6.464878	501.273854	8.396429
6.492032	501.755040	8.401446
6.083327	498.352188	8.406464
6.312640	495.171028	8.411482
6.043966	506.340001	8.416499
6.282008	506.197924	8.421517
6.164833	503.400884	8.426534
6.238972	506.359742	8.431552
6.674186	503.734207	8.436570
6.322212	497.927054	8.441587
6.713672	503.554825	8.446605
6.927999	496.293368	8.451622
6.674093	505.175612	8.456640
6.733703	499.852825	8.461658
6.599723	501.790315	8.466675
6.457411	488.607049	8.471693
6.430837	487.260454	8.476710
6.291399	504.802444	8.481728
6.641575	496.444160	8.486746
6.379543	504.884080	8.491763
6.520907	518.878265	8.496781
6.868061	508.403499	8.501798
6.583675	498.412422	8.506816
6.559693	488.991573	8.511834
6.134632	486.771267	8.516851
6.298733	498.844093	8.521869
6.477153	497.831046	8.526886
6.467458	517.150845	8.531904
6.515441	497.234570	8.536922
6.810607	504.937193	8.541939
6.244432	512.107692	8.546957
6.895983	506.024137	8.551974
6.639234	505.502212	8.556992
6.970607	516.705682	8.562010
6.634656	508.943845	8.567027
6.657012	507.126581	8.572045
6.705977	493.058549	8.577063
6.358604	489.209552	8.582080
6.658949	491.295578	8.587098
6.810456	500.764774	8.592115
6.338012	495.713935	8.597133
6.499659	506.720714	8.602151
6.594035	510.269093	8.607168
6.753622	508.453119	8.612186
6.491506	505.539342	8.617203
6.494985	511.594917	8.622221
6.558711	508.326220	8.627239
6.467581	520.282675	8.632256
6.665401	519.533915	8.637274
6.707508	514.899209	8.642291
6.654374	519.991003	8.647309
6.881623	511.008821	8.652327
6.648723	514.534234	8.657344
6.579749	514.605187	8.662362
6.343828	508.677049	8.667379
6.090134	503.846463	8.672397
6.505371	504.380899	8.677415
6.360066	508.807882	8.682432
6.435987	510.023067	8.687450
6.388923	532.706118	8.692467
6.522961	549.827901	8.697485
6.858527	544.472788	8.702503
6.851842	554.129815	8.707520
6.999834	547.557815	8.712538
7.092485	548.936953	8.717555
6.694983	532.065849	8.722573
6.824429	511.179834	8.727591
6.643091	512.480331	8.732608
6.718130	517.264503	8.737626
6.801368	533.225471	8.742643
7.005014	545.654160	8.747661
7.294410	527.021402	8.752679
6.797029	512.552320	8.757696
6.847701	507.695347	8.762714
6.760331	513.635464	8.767731
6.713424	513.119538	8.772749
6.623150	511.658498	8.777767
6.566534	510.864474	8.782784
6.766226	519.079335	8.787802
6.971487	536.716044	8.792819
6.815621	542.155935	8.797837
6.769672	536.998243	8.802855
6.934604	542.710385	8.807872
6.936653	540.728972	8.812890
6.872793	533.050996	8.817907
6.982268	545.932651	8.822925
7.377803	524.020932	8.827943
6.778021	521.516583	8.832960
6.854866	522.607411	8.837978
6.646913	511.934031	8.842995
6.657871	511.123701	8.848013
6.866017	519.285394	8.853031
7.160126	533.373779	8.858048
6.871411	524.520134	8.863066
6.958987	525.934950	8.868083
6.936445	541.121175	8.873101
6.891987	533.704928	8.878119
6.820842	532.919412	8.883136
6.960442	539.063670	8.888154
7.337379	536.720005	8.893171
6.920747	529.699223	8.898189
6.987637	517.809150	8.903207
6.745543	526.972894	8.908224
6.972692	529.623370	8.913242
7.361773	531.523460	8.918259
6.889453	529.788499	8.923277
7.308963	517.793190	8.928295
7.036316	518.396456	8.933312
6.792799	506.437131	8.938330
6.910730	504.591838	8.943347
6.721024	511.237039	8.948365
7.110118	533.207363	8.953383
7.008963	539.622771	8.958400
7.105402	535.581973	8.963418
7.428231	545.380480	8.968435
7.070911	533.639767	8.973453
7.262017	513.088594	8.978471
6.989614	514.916732	8.983488
6.459423	511.573952	8.988506
7.066841	533.772083	8.993523
7.168171	541.136965	8.998541
7.338840	536.881330	9.003559
7.224562	540.537292	9.008576
7.593510	530.209483	9.013594
7.271420	512.286812	9.018611
6.835516	511.185542	9.023629
6.818547	513.782153	9.028647
7.170088	520.258803	9.033664
7.125761	524.125013	9.038682
6.913288	528.271609	9.043699
7.183124	544.057999	9.048717
7.174811	537.685103	9.053735
7.370528	542.993750	9.058752
7.210564	533.274941	9.063770
7.346417	524.687582	9.068787
6.778612	525.076750	9.073805
7.247918	530.114318	9.078823
7.203921	543.365848	9.083840
6.830131	546.694928	9.088858
7.339148	537.487345	9.093875
7.220924	557.007436	9.098893
7.352075	543.425126	9.103911
7.512868	546.799141	9.108928
7.019499	534.860892	9.113946
7.318129	527.429763	9.118963
7.078819	546.724830	9.123981
7.350173	536.293698	9.128999
7.004748	537.145416	9.134016
6.860290	541.245519	9.139034
7.386764	540.667913	9.144051
7.195448	546.880749	9.149069
7.460895	544.761041	9.154087
7.507501	544.152272	9.159104
7.525365	542.445582	9.164122
7.589304	536.939992	9.169139
7.282518	526.126876	9.174157
7.316381	518.675031	9.179175
7.167473	524.733603	9.184192
7.125906	535.260309	9.189210
7.416451	539.760001	9.194227
7.203254	544.364957	9.199245
7.399606	545.204321	9.204263
7.257456	542.937752	9.209280
6.965262	544.138309	9.214298
7.251004	538.056067	9.219315
7.120198	544.112829	9.224333
7.537569	541.737272	9.229351
7.482916	542.433370	9.234368
7.759786	540.866064	9.239386
7.291643	541.730623	9.244403
7.376498	539.932926	9.249421
7.333557	538.829571	9.254439
7.212304	554.648647	9.259456
7.352121	545.793513	9.264474
7.652349	549.017677	9.269491
7.328824	552.403785	9.274509
7.064513	546.755708	9.279527
7.184930	540.187884	9.284544
7.313039	552.900920	9.289562
7.681151	540.969415	9.294579
7.189229	553.306413	9.299597
7.297133	547.202831	9.304615
7.379609	549.328484	9.309632
7.148980	552.282112	9.314650
7.650563	553.701994	9.319667
7.319902	558.971046	9.324685
7.421436	574.955403	9.329703
7.741059	573.348536	9.334720
7.791579	573.825068	9.339738
7.413437	556.000599	9.344755
7.129452	553.692557	9.349773
7.784859	559.949431	9.354791
7.727716	566.330399	9.359808
7.191449	556.245568	9.364826
7.946177	555.205391	9.369843
7.513605	562.128609	9.374861
7.675803	549.021631	9.379879
7.515066	548.765480	9.384896
7.240469	551.048482	9.389914
7.499552	558.252811	9.394931
7.674796	574.172013	9.399949
7.835824	573.682082	9.404967
7.825254	562.118167	9.409984
7.542406	554.259725	9.415002
7.682594	547.394156	9.420019
7.415162	552.852328	9.425037
7.449271	550.768564	9.430055
7.601227	560.834138	9.435072
7.428634	580.136308	9.440090
7.427093	579.447721	9.445107
7.585922	575.592238	9.450125
7.799388	580.478696	9.455143
7.683690	578.631925	9.460160
7.748240	586.234596	9.465178
7.805981	576.727331	9.470195
7.370651	578.581275	9.475213
8.110360	571.915615	9.480231
7.704557	567.937109	9.485248
7.756655	573.676607	9.490266
8.042483	576.077233	9.495283
7.993243	572.397139	9.500301
7.831496	562.828596	9.505319
7.742465	556.295644	9.510336
7.345388	555.999106	9.515354
7.661398	564.649030	9.520371
7.710629	570.906093	9.525389
7.868878	575.264131	9.530407
8.061707	573.789276	9.535424
7.833265	576.297300	9.540442
7.775133	558.027542	9.545459
7.732583	564.622023	9.550477
7.734997	573.887424	9.555495
8.103014	575.495161	9.560512
7.645253	567.005287	9.565530
7.715780	571.611298	9.570547
7.839321	572.748725	9.575565
7.982271	570.947310	9.580583
8.229997	564.107428	9.585600
7.739778	559.193163	9.590618
7.644437	551.059990	9.595635
7.630351	553.114434	9.600653
7.623402	567.635944	9.605671
8.070548	553.952287	9.610688
7.882619	572.572585	9.615706
7.899576	574.472099	9.620723
8.139023	583.046922	9.625741
7.850719	576.755803	9.630759
7.975601	563.743962	9.635776
7.889509	579.226948	9.640794
7.879759	585.873483	9.645811
7.691674	571.563943	9.650829
7.415177	574.811175	9.655847
7.525543	570.716884	9.660864
7.636329	585.758248	9.665882
7.683308	575.016629	9.670899
7.612886	578.238398	9.675917
7.787176	580.296888	9.680935
8.039423	586.379208	9.685952
8.074572	600.259568	9.690970
7.915911	592.391762	9.695987
8.118569	593.882798	9.701005
8.019846	591.192522	9.706023
8.269335	582.319797	9.711040
7.914649	583.487204	9.716058
8.098195	578.218470	9.721075
8.074883	570.971527	9.726093
7.608581	575.105642	9.731111
8.048611	589.424033	9.736128
7.886153	599.747390	9.741146
8.323210	607.410428	9.746163
8.210230	614.202801	9.751181
8.342764	608.091967	9.756199
8.542544	580.140145	9.761216
8.042986	581.722066	9.766234
7.721385	576.769246	9.771251
8.291309	584.029785	9.776269
7.988570	572.822488	9.781287
8.351138	571.525221	9.786304
8.051355	570.189610	9.791322
8.183004	574.350294	9.796339
7.922225	569.088803	9.801357
7.794235	576.618831	9.806375
7.939071	588.861244	9.811392
7.959841	605.075527	9.816410
8.389740	606.681879	9.821427
8.682645	608.885287	9.826445
8.535855	605.672490	9.831463
8.331310	580.264427	9.836480
8.076254	579.088917	9.841498
8.161533	570.271932	9.846515
8.190821	569.114098	9.851533
7.929293	573.279851	9.856551
8.259023	574.538441	9.861568
7.862231	590.390975	9.866586
8.438416	596.137591	9.871603
8.243432	596.744534	9.876621
8.601544	605.070404	9.881639
8.486982	585.875373	9.886656
8.172406	574.742865	9.891674
7.917992	563.345695	9.896691
8.260226	585.841338	9.901709
8.264730	596.405140	9.906727
8.572361	595.749406	9.911744
8.435788	595.553619	9.916762
8.244425	580.787557	9.921779
8.405802	570.840328	9.926797
8.153244	571.937480	9.931815
8.170879	588.437089	9.936832
8.179109	605.153218	9.941850
8.402923	595.319840	9.946867
8.677144	600.318481	9.951885
8.338809	599.991153	9.956903
8.413150	602.964365	9.961920
8.368112	604.398786	9.966938
8.434026	606.426803	9.971955
8.398919	596.641416	9.976973
8.240365	604.875685	9.981991
8.423565	600.130982	9.987008
8.365440	595.244953	9.992026
8.494156	599.702960	9.997043
8.390498	604.488995	10.002061
8.257671	603.720381	10.007079
8.614655	593.026622	10.012096
8.455821	602.003997	10.017114
8.766848	602.899372	10.022131
8.650177	594.554367	10.027149
8.170690	600.166165	10.032167
8.348580	606.656253	10.037184
8.529158	605.566666	10.042202
8.233242	603.791857	10.047219
8.593350	598.888341	10.052237
8.378243	602.558849	10.057255
8.300135	603.392289	10.062272
8.519453	612.171433	10.067290
8.433902	601.639720	10.072307
8.633590	601.891762	10.077325
8.203751	607.860476	10.082343
8.449921	608.801234	10.087360
8.266001	608.907755	10.092378
8.083720	600.473815	10.097395
8.680787	596.905776	10.102413
8.310405	604.313957	10.107431
8.471787	615.406285	10.112448
8.526409	625.614389	10.117466
8.745378	633.326150	10.122483
9.038747	631.957271	10.127501
8.553383	623.511107	10.132519
8.475370	609.531315	10.137536
9.025360	621.166740	10.142554
8.443714	610.946877	10.147571
8.674509	605.526027	10.152589
8.348346	616.095190	10.157607
8.894377	619.695569	10.162624
8.698760	630.828914	10.167642
8.670795	631.907973	10.172659
8.950335	618.644508	10.177677
8.446854	621.064429	10.182695
8.642658	617.314617	10.187712
8.738466	630.495240	10.192730
8.809747	637.465759	10.197747
9.078518	623.299405	10.202765
8.838767	615.833770	10.207783
8.802766	609.953192	10.212800
8.661225	601.339682	10.217818
8.644890	599.148130	10.222835
8.826702	600.335355	10.227853
8.575839	612.257114	10.232871
8.701970	625.416965	10.237888
8.512231	627.005852	10.242906
8.693491	631.898840	10.247923
8.802951	621.843254	10.252941
8.265520	635.840109	10.257959
8.499537	630.958053	10.262976
8.971624	633.701838	10.267994
8.534667	638.972770	10.273011
8.463492	641.741163	10.278029
8.806316	633.685383	10.283047
8.786398	635.966183	10.288064
8.912447	636.494183	10.293082
8.684339	639.450756	10.298099
9.101374	647.476950	10.303117
8.660080	647.518616	10.308135
9.105297	653.663886	10.313152
9.192395	654.847509	10.318170
8.807904	646.000007	10.323187
9.105163	632.679268	10.328205
8.760723	632.032892	10.333223
8.886498	637.120885	10.338240
9.102894	638.846447	10.343258
9.136101	640.361412	10.348275
9.050845	636.718368	10.353293
9.005491	636.399215	10.358311
8.910436	628.787180	10.363328
9.080954	631.460435	10.368346
8.826149	631.177539	10.373363
8.860656	629.446826	10.378381
9.083650	638.397215	10.383399
9.110745	649.172455	10.388416
9.198736	637.204786	10.393434
9.150358	644.974601	10.398451
9.246124	629.199197	10.403469
8.939479	630.923970	10.408487
8.735020	625.475192	10.413504
9.073814	640.748129	10.418522
9.173437	653.570682	10.423539
9.085386	648.421892	10.428557
9.213898	652.551622	10.433575
9.184427	646.027076	10.438592
8.978981	634.420184	10.443610
8.523287	647.352006	10.448627
8.900711	653.843914	10.453645
9.426404	664.662974	10.458663
9.496057	663.896850	10.463680
9.496279	662.450533	10.468698
9.034265	665.502532	10.473715
9.064140	664.730791	10.478733
9.262584	669.420171	10.483751
9.321044	659.781248	10.488768
9.196627	664.446140	10.493786
9.234739	672.881921	10.498803
9.287887	659.490957	10.503821
9.273716	654.339380	10.508839
8.704607	655.739136	10.513856
9.475020	651.990618	10.518874
9.266799	657.663418	10.523891
9.460889	656.512932	10.528909
9.235824	657.410471	10.533927
9.262307	659.864289	10.538944
9.405652	659.380433	10.543962
9.429098	662.291026	10.548979
9.522823	654.072164	10.553997
9.044748	638.088641	10.559015
9.108532	649.084169	10.564032
9.582027	644.275833	10.569050
9.393921	658.377453	10.574067
9.418882	641.772474	10.579085
9.457718	642.731031	10.584103
9.104607	633.536630	10.589120
9.067323	640.444030	10.594138
9.198088	650.409635	10.599155
9.288764	657.015163	10.604173
9.286680	661.294859	10.609191
9.419664	668.855532	10.614208
9.334074	662.529237	10.619226
9.204643	676.706191	10.624243
9.401751	662.052487	10.629261
9.447451	665.687303	10.634279
9.553517	659.180069	10.639296
9.351042	658.697575	10.644314
9.714059	667.885408	10.649331
9.546392	658.991761	10.654349
9.654819	661.983158	10.659367
9.550113	669.312340	10.664384
10.004323	653.225604	10.669402
9.500469	669.918337	10.674419
9.581064	662.141382	10.679437
9.628177	663.954029	10.684455
9.610915	666.356435	10.689472
9.737502	651.079811	10.694490
9.224778	654.745679	10.699507
9.660677	656.832902	10.704525
9.809844	658.052308	10.709543
9.518095	660.804475	10.714560
9.469628	638.732075	10.719578
9.467392	662.377911	10.724595
9.483915	655.685912	10.729613
9.283205	663.053428	10.734631
9.241355	658.700872	10.739648
9.659484	659.330499	10.744666
9.450352	660.003759	10.749683
9.390874	662.269856	10.754701
9.386011	664.381643	10.759719
9.167280	659.508803	10.764736
9.291515	655.131896	10.769754
9.565404	676.263679	10.774771
9.605744	683.873163	10.779789
9.696688	680.187940	10.784807
10.124639	694.000191	10.789824
10.031907	680.316849	10.794842
9.861703	677.499623	10.799859
9.429294	669.498575	10.804877
9.472034	674.110202	10.809895
9.620583	683.918168	10.814912
10.154122	687.637948	10.819930
9.669695	674.896189	10.824947
9.685430	669.079065	10.829965
9.535578	675.926780	10.834983
9.558483	688.586879	10.840000
9.810850	679.503989	10.845018
9.633358	684.858737	10.850035
9.836036	682.495483	10.855053
9.843785	687.821920	10.860071
9.616665	690.876365	10.865088
9.872628	682.721169	10.870106
10.005437	686.402193	10.875123
9.978609	682.249886	10.880141
9.893293	675.507817	10.885159
9.888073	686.772657	10.890176
9.906706	682.624633	10.895194
9.909537	681.690843	10.900211
9.778365	678.093185	10.905229
9.958511	684.039067	10.910247
9.662368	693.447475	10.915264
9.968372	681.547996	10.920282
9.966288	682.320430	10.925299
9.953732	686.203072	10.930317
10.107682	683.045179	10.935335
9.649917	686.035852	10.940352
9.977870	683.613273	10.945370
9.705072	686.990223	10.950387
9.848989	686.915695	10.955405
9.888132	679.756976	10.960423
9.744269	682.951954	10.965440
9.550340	681.319294	10.970458
9.873105	700.152604	10.975475
10.089072	719.113064	10.980493
10.005339	716.670072	10.985511
10.237308	718.401332	10.990528
10.653108	712.676598	10.995546
10.124118	701.437778	11.000563
9.973844	694.573787	11.005581
10.258729	688.841608	11.010599
9.969610	686.651122	11.015616
10.148172	682.876591	11.020634
10.163605	682.941049	11.025651
10.158892	683.549754	11.030669
10.158366	683.555834	11.035687
10.217212	690.234360	11.040704
10.248030	685.483566	11.045722
10.126553	676.764138	11.050739
9.855177	686.279458	11.055757
10.283481	674.683336	11.060775
9.789815	693.479003	11.065792
10.098272	711.029733	11.070810
10.068305	716.737207	11.075827
10.263343	722.441281	11.080845
10.351173	713.907634	11.085863
10.401100	716.240657	11.090880
10.040225	710.833103	11.095898
10.233668	716.722862	11.100915
10.286202	723.078843	11.105933
10.457025	714.128721	11.110951
10.500713	718.261885	11.115968
10.511866	721.301683	11.120986
10.382009	706.144629	11.126003
10.145582	694.597149	11.131021
10.438288	700.613370	11.136039
10.310983	706.784963	11.141056
10.456740	704.242166	11.146074
9.990446	699.742570	11.151091
9.923702	709.508648	11.156109
10.092622	711.733390	11.161127
10.207062	711.354706	11.166144
9.994463	710.903412	11.171162
10.114532	721.130267	11.176179
10.034781	723.496574	11.181197
10.325075	716.585211	11.186215
10.403505	713.362656	11.191232
10.544300	702.392827	11.196250
10.102419	718.945437	11.201267
9.983679	730.954654	11.206285
10.728213	728.794172	11.211303
10.687789	735.356485	11.216320
10.513840	737.573442	11.221338
10.559359	737.975418	11.226355
10.690968	738.372587	11.231373
10.537108	721.951060	11.236391
10.669834	737.877865	11.241408
10.910906	718.483631	11.246426
10.781921	717.311839	11.251443
10.361527	709.600496	11.256461
10.506313	703.426183	11.261479
10.784050	713.627319	11.266496
10.807787	709.081615	11.271514
10.705853	713.485728	11.276531
10.430747	711.428736	11.281549
10.287441	706.125700	11.286567
10.158325	710.255588	11.291584
10.583265	717.470714	11.296602
10.934587	725.248002	11.301619
10.565983	734.420810	11.306637
10.825729	716.708824	11.311655
10.479179	713.196031	11.316672
10.427678	727.930174	11.321690
11.013509	730.236661	11.326707
11.057453	726.965093	11.331725
11.074565	712.046281	11.336743
10.614323	713.683905	11.341760
10.885402	705.909636	11.346778
10.582936	706.718425	11.351795
10.641343	710.555073	11.356813
10.738417	706.510582	11.361831
10.651987	716.444875	11.366848
10.651213	711.404834	11.371866
10.838823	718.161256	11.376883
10.710445	715.433155	11.381901
10.881910	708.062366	11.386919
10.464109	714.279308	11.391936
11.021173	729.876013	11.396954
10.659982	734.831693	11.401971
10.558937	739.165590	11.406989
10.680647	737.976693	11.412007
10.945848	742.936128	11.417024
11.135948	745.282163	11.422042
11.318612	737.207576	11.427059
10.951440	737.192877	11.432077
10.940345	731.845500	11.437095
10.982448	721.477399	11.442112
10.820727	719.518554	11.447130
10.678072	733.637517	11.452147
10.759467	737.404621	11.457165
11.123966	729.682585	11.462183
11.211976	742.881522	11.467200
11.167909	737.741167	11.472218
11.072100	738.604315	11.477235
11.131429	729.562809	11.482253
11.145950	715.062116	11.487271
11.050006	714.535209	11.492288
10.693398	709.677704	11.497306
11.096559	711.622727	11.502323
10.794363	714.255775	11.507341
11.452064	721.202453	11.512359
11.149482	719.953901	11.517376
11.080720	712.366603	11.522394
11.166481	713.665012	11.527411
11.160594	716.371429	11.532429
11.063221	706.211857	11.537447
10.990645	709.186781	11.542464
11.069249	701.236130	11.547482
11.611944	703.846196	11.552499
11.249033	706.940844	11.557517
11.247801	700.362783	11.562535
10.918419	707.829574	11.567552
10.796657	710.703201	11.572570
11.303459	712.203922	11.577587
11.198942	707.445218	11.582605
11.035461	703.369468	11.587623
11.173486	713.179589	11.592640
11.302257	726.487898	11.597658
11.202786	720.143406	11.602675
11.297072	739.778727	11.607693
11.408497	743.331423	11.612711
11.320560	736.413393	11.617728
11.019691	725.554868	11.622746
11.593195	717.839565	11.627763
11.196710	724.924192	11.632781
11.546857	722.364475	11.637799
11.538046	713.238205	11.642816
10.964881	717.262894	11.647834
11.272972	706.350395	11.652851
11.144336	724.422703	11.657869
11.418075	732.391571	11.662887
11.331578	737.643479	11.667904
11.358037	735.670006	11.672922
11.438658	730.723954	11.677939
11.323189	741.284690	11.682957
11.428265	738.512022	11.687975
11.325495	739.078703	11.692992
11.335773	738.979063	11.698010
11.439863	739.295360	11.703027
11.412488	732.145269	11.708045
11.775092	735.587871	11.713063
11.311784	737.402373	11.718080
11.445381	739.251887	11.723098
11.702938	741.443453	11.728115
11.558920	737.854206	11.733133
11.759967	729.674223	11.738151
11.622724	733.679880	11.743168
11.606802	742.023470	11.748186
11.468469	734.924427	11.753203
11.454303	745.710897	11.758221
11.368527	742.216330	11.763239
11.525125	743.659696	11.768256
11.376408	738.260306	11.773274
11.702411	729.550212	11.778291
11.234926	742.157312	11.783309
11.569658	742.545255	11.788327
11.476463	734.982464	11.793344
11.229343	736.763924	11.798362
11.843145	727.627850	11.803379
11.449228	733.373156	11.808397
11.447022	745.811094	11.813415
11.381532	742.195065	11.818432
11.629648	739.875063	11.823450
11.686179	742.408560	11.828467
11.558431	746.696884	11.833485
11.957918	761.547316	11.838503
12.105485	754.032045	11.843520
11.818201	737.894785	11.848538
11.980473	735.206342	11.853555
11.517023	741.379676	11.858573
11.714074	741.806558	11.863591
11.530724	741.681897	11.868608
11.601555	744.553952	11.873626
12.087150	754.590389	11.878643
11.928525	762.289153	11.883661
11.761262	748.315353	11.888679
11.776895	743.929240	11.893696
11.823504	747.144657	11.898714
11.851498	761.980623	11.903731
11.958538	763.887291	11.908749
12.158028	761.255276	11.913767
11.821418	746.823719	11.918784
11.537870	755.960408	11.923802
11.895802	759.784871	11.928819
11.646178	775.564408	11.933837
11.929847	761.791503	11.938855
12.187268	765.466084	11.943872
11.931851	774.075714	11.948890
12.118946	767.582575	11.953907
11.859828	776.698304	11.958925
11.916086	767.206915	11.963943
12.023961	772.312877	11.968960
11.853548	775.868156	11.973978
12.122060	766.563263	11.978995
11.527922	777.807188	11.984013
11.863155	772.013889	11.989031
11.946409	771.370304	11.994048
11.963754	771.088795	11.999066
12.336077	765.228336	12.004083
12.112260	772.520993	12.009101
12.146846	768.121500	12.014119
12.157325	772.500715	12.019136
11.846794	774.046236	12.024154
12.151180	767.154563	12.029171
11.988013	772.168011	12.034189
12.186145	770.319248	12.039207
12.093504	762.873667	12.044224
11.938043	768.968456	12.049242
11.964077	768.277262	12.054259
12.186576	790.102319	12.059277
12.369392	787.860049	12.064295
12.556330	791.491192	12.069312
12.222221	789.212476	12.074330
12.408407	776.443442	12.079347
12.469499	773.022969	12.084365
12.186785	767.180822	12.089383
12.312733	764.676726	12.094400
12.126111	766.958380	12.099418
12.527842	759.913590	12.104435
12.482949	766.229032	12.109453
12.440887	762.197331	12.114471
12.406534	761.791712	12.119488
12.182035	764.058773	12.124506
12.322992	762.730473	12.129523
12.407759	759.476152	12.134541
12.125464	759.378504	12.139559
12.331826	775.356931	12.144576
12.442410	790.071380	12.149594
12.653026	796.415781	12.154611
12.591776	785.417936	12.159629
12.899270	777.647050	12.164647
12.238302	769.594037	12.169664
12.226014	774.027414	12.174682
12.487497	768.357739	12.179699
12.416345	759.925978	12.184717
12.101980	773.339593	12.189735
12.349897	782.165079	12.194752
12.364740	793.965228	12.199770
12.851997	790.643466	12.204787
12.342256	797.428392	12.209805
12.909507	796.962130	12.214823
12.666274	797.315076	12.219840
12.687424	798.921419	12.224858
12.750818	790.100059	12.229875
12.814304	798.997824	12.234893
12.369320	781.336320	12.239911
12.830846	789.255226	12.244928
12.859428	788.530934	12.249946
12.766356	779.186306	12.254963
12.766719	767.321231	12.259981
12.588526	769.587711	12.264999
12.437493	768.336106	12.270016
12.351383	784.799955	12.275034
12.327402	784.943376	12.280051
12.525365	797.063974	12.285069
12.458600	801.758335	12.290087
12.659712	798.265461	12.295104
12.420874	801.846250	12.300122
12.697452	792.440798	12.305139
12.626589	795.371757	12.310157
12.627278	795.449679	12.315175
13.077810	793.876819	12.320192
12.851892	803.075250	12.325210
12.980370	801.520679	12.330227
12.932380	791.481214	12.335245
12.949807	799.047306	12.340263
13.036999	796.903541	12.345280
12.696110	798.200561	12.350298
12.810930	790.232452	12.355315
12.928776	800.960488	12.360333
12.987612	796.174708	12.365351
13.167531	788.116690	12.370368
13.024527	798.936341	12.375386
13.034390	787.665315	12.380403
13.140066	796.423029	12.385421
13.338925	795.068211	12.390439
13.185992	788.720733	12.395456
12.877019	792.367066	12.400474
13.008797	789.321873	12.405491
13.130488	796.775429	12.410509
12.531777	789.429381	12.415527
13.068170	790.431930	12.420544
12.995701	794.839060	12.425562
12.724160	791.202811	12.430579
12.941262	788.038770	12.435597
12.878884	794.376409	12.440615
13.137113	803.844260	12.445632
13.068457	823.202746	12.450650
13.341477	816.320575	12.455667
13.018412	803.366567	12.460685
13.065457	816.127886	12.465703
13.539446	810.268291	12.470720
13.090969	811.610291	12.475738
13.214360	792.888960	12.480755
13.511498	790.285258	12.485773
12.733351	790.747249	12.490791
13.387632	800.336909	12.495808
13.323621	817.122313	12.500826
13.485626	806.229997	12.505843
13.443930	801.641954	12.510861
13.129638	799.633957	12.515879
13.186714	783.800632	12.520896
13.012977	805.466530	12.525914
13.467369	813.672442	12.530931
13.762566	821.026418	12.535949
13.204326	799.876346	12.540967
13.217769	796.258257	12.545984
12.869211	799.925713	12.551002
13.196013	813.607978	12.556019
13.368708	814.263686	12.561037
13.532536	829.311858	12.566055
13.881521	808.428458	12.571072
13.341452	817.787179	12.576090
13.298281	826.279020	12.581107
13.719699	826.403018	12.586125
13.382863	833.356562	12.591143
13.457353	820.799285	12.596160
13.436439	823.950706	12.601178
13.287457	816.080593	12.606195
13.429947	817.534570	12.611213
13.103613	821.971933	12.616231
13.449764	814.948133	12.621248
13.633930	822.143338	12.626266
13.570759	823.305402	12.631283
13.757333	816.008040	12.636301
13.283564	826.967909	12.641319
13.695184	817.062547	12.646336
13.258174	820.483251	12.651354
13.668754	817.574947	12.656371
13.874983	811.433328	12.661389
13.927328	816.163479	12.666407
13.985709	816.214133	12.671424
13.666459	828.094038	12.676442
13.676486	825.505983	12.681459
13.811563	818.737593	12.686477
13.548086	818.827369	12.691495
13.336439	822.985913	12.696512
13.452502	822.702229	12.701530
13.328027	824.263401	12.706547
13.643501	822.899113	12.711565
13.747184	838.822563	12.716583
14.027364	840.865917	12.721600
13.772350	849.499930	12.726618
13.930153	844.337528	12.731635
13.955650	843.503514	12.736653
13.686902	849.346240	12.741671
13.732021	834.409288	12.746688
13.784830	847.046849	12.751706
14.072280	841.264192	12.756723
14.302490	841.524177	12.761741
13.857732	834.038054	12.766759
13.825497	827.233588	12.771776
13.992072	831.104714	12.776794
13.958500	834.937727	12.781811
14.385499	834.900573	12.786829
13.969565	825.201525	12.791847
13.859316	810.947374	12.796864
13.715169	818.712663	12.801882
14.190410	832.964430	12.806899
14.067985	834.926424	12.811917
13.816021	849.144691	12.816935
14.333328	844.308568	12.821952
14.101681	846.877990	12.826970
14.053823	839.826512	12.831987
14.319615	829.227215	12.837005
14.338553	825.256258	12.842023
14.302394	812.277962	12.847040
14.112112	811.811159	12.852058
13.990325	816.951226	12.857075
14.076605	807.578851	12.862093
14.150377	814.288028	12.867111
14.259563	806.246438	12.872128
14.398446	809.659176	12.877146
13.904138	812.508293	12.882163
14.243935	815.753126	12.887181
14.094907	839.525108	12.892199
14.181429	833.612347	12.897216
14.008257	844.853146	12.902234
14.224332	835.592720	12.907251
14.059508	839.925790	12.912269
14.332188	836.111623	12.917287
14.309524	834.898596	12.922304
14.525612	840.927559	12.927322
14.539609	842.209911	12.932339
14.440032	837.936544	12.937357
14.438500	837.873503	12.942375
14.449155	836.246712	12.947392
14.581022	845.505209	12.952410
14.675213	845.194833	12.957427
14.795067	835.023220	12.962445
14.280061	816.291829	12.967463
14.361458	819.738496	12.972480
14.389122	832.524690	12.977498
14.563069	842.767113	12.982515
14.728704	834.349643	12.987533
14.613146	836.110904	12.992551
14.277345	820.764622	12.997568
14.806056	830.862865	13.002586
14.250680	835.346032	13.007603
15.046469	841.343568	13.012621
14.506393	829.978937	13.017639
14.622477	816.589621	13.022656
14.609228	810.359154	13.027674
14.545890	812.092081	13.032691
14.833458	816.975399	13.037709
14.628450	815.537856	13.042727
14.297911	811.673588	13.047744
14.709722	819.023213	13.052762
14.320337	850.739726	13.057779
14.809959	839.696686	13.062797
14.529856	852.536614	13.067815
14.894692	832.195806	13.072832
14.661095	842.502169	13.077850
14.375579	845.366323	13.082867
14.555842	834.876455	13.087885
14.658823	840.063560	13.092903
14.793816	834.699831	13.097920
14.894255	836.405248	13.102938
14.514508	840.761309	13.107955
14.765276	830.921941	13.112973
14.472825	842.060448	13.117991
14.540755	846.139635	13.123008
14.528558	846.606680	13.128026
14.475629	865.416972	13.133043
15.182645	851.244770	13.138061
15.314738	858.567507	13.143079
15.507664	855.681851	13.148096
15.544954	848.461159	13.153114
15.181972	836.024731	13.158131
15.391633	819.264181	13.163149
15.002304	823.466713	13.168167
15.222745	816.842842	13.173184
15.288907	820.730593	13.178202
15.009050	819.165292	13.183219
15.350936	814.782220	13.188237
15.369071	813.941553	13.193255
15.489488	816.631404	13.198272
15.216033	803.131413	13.203290
14.846683	799.388923	13.208307
15.216262	808.856449	13.213325
15.187544	813.308699	13.218343
15.417490	812.693182	13.223360
15.293573	800.968339	13.228378
14.845664	802.400003	13.233395
15.185662	798.007012	13.238413
15.305205	802.020164	13.243431
15.068197	816.218603	13.248448
15.226917	810.943074	13.253466
15.108590	819.132412	13.258483
15.190784	820.415673	13.263501
15.201627	828.390724	13.268519
15.141069	825.910808	13.273536
15.379255	822.059840	13.278554
15.140245	822.069978	13.283571
15.099267	816.393679	13.288589
15.288728	826.412274	13.293607
14.968807	817.938213	13.298624
15.325755	823.901328	13.303642
15.076908	828.610493	13.308659
15.078444	819.751330	13.313677
15.185065	832.500436	13.318695
15.404277	841.133475	13.323712
15.583506	848.795628	13.328730
15.192358	855.116082	13.333747
15.328768	855.897086	13.338765
15.312415	857.877738	13.343783
15.301975	852.814055	13.348800
15.519387	863.536278	13.353818
15.320014	859.299902	13.358835
15.589490	855.879155	13.363853
15.866007	858.692371	13.368871
15.110057	860.270318	13.373888
15.934968	848.619418	13.378906
15.860818	855.570812	13.383923
15.978028	854.190929	13.388941
15.704102	862.453690	13.393959
15.605451	857.732155	13.398976
15.617996	845.587850	13.403994
15.472844	856.469312	13.409011
15.491243	849.169074	13.414029
15.580056	855.412809	13.419047
15.431687	853.947774	13.424064
15.580511	856.332156	13.429082
15.288578	858.073020	13.434099
15.736785	858.437453	13.439117
15.616738	858.070430	13.444135
15.663463	873.867134	13.449152
15.804715	875.605559	13.454170
16.028474	875.756776	13.459187
16.371975	870.524643	13.464205
16.095710	863.193667	13.469223
15.850394	856.491791	13.474240
16.033050	849.713540	13.479258
15.400800	857.449047	13.484275
15.833103	847.148921	13.489293
15.613973	854.349901	13.494311
15.902918	866.079522	13.499328
16.081760	869.227009	13.504346
15.909843	885.259919	13.509363
16.214106	878.246175	13.514381
16.336700	876.044178	13.519399
15.928590	863.730942	13.524416
15.703914	863.070236	13.529434
15.782020	876.926802	13.534451
15.921927	878.789066	13.539469
16.166011	885.777932	13.544487
16.093672	886.156910	13.549504
16.334006	873.951638	13.554522
16.222671	876.330285	13.559539
16.216230	883.383860	13.564557
16.508987	877.540471	13.569575
16.275345	880.256285	13.574592
16.349058	878.126157	13.579610
16.392351	880.946895	13.584627
16.314994	864.053516	13.589645
16.021833	854.576627	13.594663
16.004561	861.140278	13.599680
16.565740	865.107482	13.604698
16.254509	873.440990	13.609715
16.422725	875.148180	13.614733
16.358628	875.159275	13.619751
16.200324	880.452254	13.624768
16.385083	880.056411	13.629786
16.487031	882.346595	13.634803
16.287660	879.699902	13.639821
16.528216	878.639340	13.644839
16.244213	883.032705	13.649856
16.465044	877.733484	13.654874
16.285742	884.863318	13.659891
16.316941	875.392154	13.664909
16.264194	877.979200	13.669927
16.349715	879.006809	13.674944
16.417075	878.528443	13.679962
16.274205	879.573005	13.684979
16.341249	877.660507	13.689997
16.324864	878.732942	13.695015
15.925915	881.244250	13.700032
16.281046	877.844353	13.705050
16.485179	895.613739	13.710067
16.768518	912.013005	13.715085
16.644275	901.416829	13.720103
16.697157	906.610677	13.725120
16.789979	899.446905	13.730138
16.772025	894.286032	13.735155
16.921998	891.742113	13.740173
16.914710	876.799230	13.745191
16.678495	875.758956	13.750208
16.817663	858.012446	13.755226
16.903681	864.984171	13.760243
16.401663	870.893876	13.765261
16.927681	882.213406	13.770279
16.612487	890.490889	13.775296
16.720690	894.466181	13.780314
16.598908	905.657178	13.785331
16.619192	910.808396	13.790349
17.049403	901.130601	13.795367
16.696726	902.097706	13.800384
16.846686	903.081184	13.805402
16.911592	901.219429	13.810419
17.104054	897.763790	13.815437
16.964513	903.331216	13.820455
16.964201	904.926164	13.825472
16.893198	892.757470	13.830490
17.281793	903.719080	13.835507
17.140056	897.624416	13.840525
17.277150	892.588650	13.845543
16.961905	900.304756	13.850560
17.100715	887.247426	13.855578
16.828945	898.936854	13.860595
17.081806	902.196888	13.865613
17.421525	900.783699	13.870631
17.105939	900.725025	13.875648
17.031963	895.612403	13.880666
16.987404	895.360432	13.885683
17.070111	891.723765	13.890701
16.928391	892.300444	13.895719
17.113695	895.224435	13.900736
17.239265	882.773604	13.905754
17.196670	895.492354	13.910771
17.167512	889.766435	13.915789
17.508382	894.902751	13.920807
17.309209	890.679718	13.925824
17.128439	893.335600	13.930842
17.124657	893.491032	13.935859
17.213961	890.062712	13.940877
17.340872	889.930767	13.945895
17.109212	888.048832	13.950912
17.213119	884.181501	13.955930
17.124445	886.986298	13.960947
17.285549	883.524439	13.965965
17.476816	890.809441	13.970983
17.630064	899.568390	13.976000
17.398160	893.909111	13.981018
17.737800	886.559600	13.986035
17.702091	893.628262	13.991053
17.514698	886.226263	13.996071
17.181661	890.284065	14.001088
17.655953	887.489603	14.006106
17.518498	887.345530	14.011123
17.705878	896.055127	14.016141
17.737242	887.607896	14.021159
17.669025	884.931217	14.026176
17.755925	880.043130	14.031194
17.820560	878.593214	14.036211
17.230910	877.905149	14.041229
17.697047	878.218584	14.046247
17.494933	895.353697	14.051264
17.837101	906.497398	14.056282
17.807328	898.513413	14.061299
17.838421	903.235300	14.066317
17.941497	902.222303	14.071335
17.768882	899.538106	14.076352
17.422305	892.854556	14.081370
17.650054	898.124953	14.086387
17.912723	901.514066	14.091405
17.932130	902.573883	14.096423
17.610848	913.375893	14.101440
17.910176	901.087606	14.106458
18.092356	906.515544	14.111475
17.760064	910.078762	14.116493
17.937607	899.888894	14.121511
18.096809	908.238220	14.126528
18.362611	899.547054	14.131546
18.141323	899.807002	14.136563
18.039276	898.953949	14.141581
18.185658	904.722445	14.146599
18.039001	906.399891	14.151616
17.983315	905.467116	14.156634
17.812466	899.787095	14.161651
17.919407	898.659290	14.166669
18.274020	897.964469	14.171687
18.317868	905.366010	14.176704
18.355986	904.545650	14.181722
18.342583	904.607797	14.186739
17.861888	907.544830	14.191757
18.299864	901.733682	14.196775
17.966698	912.682534	14.201792
17.825511	910.217531	14.206810
18.542814	909.182351	14.211827
18.523588	914.558606	14.216845
18.590463	904.292576	14.221863
18.678444	903.827723	14.226880
18.148428	889.641038	14.231898
18.307284	883.527313	14.236915
18.183044	892.380235	14.241933
18.345591	891.834928	14.246951
18.026204	905.187286	14.251968
18.458389	900.496732	14.256986
18.505037	903.656667	14.262003
18.191826	908.925308	14.267021
18.248496	908.699093	14.272039
18.445074	904.112114	14.277056
18.003824	911.706183	14.282074
18.326441	906.550327	14.287091
18.292747	912.480133	14.292109
18.431297	907.471680	14.297127
18.178699	906.693552	14.302144
18.577630	916.988530	14.307162
18.828425	928.166274	14.312179
18.485922	920.728133	14.317197
18.477940	910.344185	14.322215
18.738045	916.345812	14.327232
18.965352	931.536322	14.332250
18.711718	914.786638	14.337267
18.639861	919.218897	14.342285
18.777673	905.443640	14.347303
18.691036	916.641817	14.352320
18.510088	923.073155	14.357338
18.807322	934.371554	14.362355
18.865008	940.261044	14.367373
19.084743	946.513451	14.372391
19.084416	921.660355	14.377408
18.656548	928.112897	14.382426
18.782198	915.859655	14.387443
18.657333	929.805387	14.392461
19.074381	924.134305	14.397479
19.006014	943.370064	14.402496
19.084734	926.638560	14.407514
18.838522	913.633545	14.412531
18.957393	934.296885	14.417549
19.064046	933.286837	14.422567
18.822225	937.546860	14.427584
18.916456	941.964616	14.432602
19.280688	935.310193	14.437619
18.920685	946.731602	14.442637
18.844826	940.324450	14.447655
18.719949	944.082455	14.452672
18.880139	929.249973	14.457690
19.261201	927.392948	14.462707
19.287669	936.251648	14.467725
19.342522	941.968388	14.472743
19.472584	934.832683	14.477760
19.678163	931.599658	14.482778
19.459507	937.756943	14.487795
19.079939	935.447938	14.492813
19.355245	930.856183	14.497831
19.564267	933.249506	14.502848
19.437501	931.896629	14.507866
19.613291	908.098597	14.512883
19.043832	908.382339	14.517901
18.891235	905.344449	14.522919
19.227617	914.097098	14.527936
19.055582	932.218958	14.532954
19.319434	926.164992	14.537971
19.086879	935.521680	14.542989
19.469206	930.792131	14.548007
19.570166	928.521270	14.553024
19.444791	929.845210	14.558042
19.511409	928.579598	14.563059
19.219300	930.577575	14.568077
19.213135	931.154248	14.573095
19.350357	930.709586	14.578112
19.123283	929.210727	14.583130
19.470602	937.977326	14.588147
19.571750	955.833516	14.593165
19.704937	963.097856	14.598183
19.999991	964.944677	14.603200
19.673044	954.345416	14.608218
19.726545	934.684346	14.613235
19.366849	939.580003	14.618253
19.800712	941.601859	14.623271
19.868238	952.674540	14.628288
19.764062	954.727618	14.633306
19.767220	945.004371	14.638323
19.764366	961.932949	14.643341
19.896384	955.981113	14.648359
19.597286	951.982081	14.653376
19.974490	965.222295	14.658394
19.957077	949.353499	14.663411
19.683717	963.447073	14.668429
19.663398	957.722421	14.673447
20.080067	945.292627	14.678464
19.918657	959.751502	14.683482
20.114946	967.725050	14.688499
19.624953	956.676427	14.693517
19.677468	963.384464	14.698535
19.880323	955.668217	14.703552
19.647443	962.007386	14.708570
19.814131	956.466721	14.713587
19.900799	953.207714	14.718605
19.860021	960.939817	14.723623
20.176771	967.867084	14.728640
20.019405	985.129526	14.733658
20.415710	984.101826	14.738675
20.557188	984.227694	14.743693
20.541008	974.463933	14.748711
20.452349	955.237777	14.753728
20.255264	961.559208	14.758746
20.331952	951.415533	14.763763
19.977887	959.259350	14.768781
20.267872	946.461178	14.773799
20.201661	946.803711	14.778816
20.275484	951.525230	14.783834
20.474289	944.205311	14.788851
20.255237	952.873976	14.793869
20.296668	956.283593	14.798887
20.299458	955.092325	14.803904
20.231809	976.749558	14.808922
20.641279	980.332088	14.813939
20.429434	985.734751	14.818957
20.412948	978.667779	14.823975
20.542958	978.627442	14.828992
20.557424	982.708038	14.834010
20.848793	976.426277	14.839027
20.776046	981.249631	14.844045
20.657755	963.863728	14.849063
20.941040	951.013909	14.854080
20.464337	948.211165	14.859098
20.376265	938.938050	14.864115
20.621958	948.919462	14.869133
20.448468	965.098378	14.874151
20.863665	960.961383	14.879168
20.880736	978.955139	14.884186
20.979156	960.761341	14.889203
20.811836	954.514597	14.894221
20.826234	942.752177	14.899239
20.794684	940.648525	14.904256
20.704897	946.731328	14.909274
20.861235	946.668129	14.914291
20.737256	947.469421	14.919309
21.003940	957.539090	14.924327
21.158340	960.412308	14.929344
20.741360	959.288578	14.934362
20.940773	949.772980	14.939379
20.956942	954.781593	14.944397
21.078640	967.018099	14.949415
21.495381	965.008711	14.954432
20.928168	943.063110	14.959450
20.961986	934.726465	14.964467
20.826329	942.058933	14.969485
20.974397	954.206814	14.974503
20.915301	964.498141	14.979520
21.077412	974.504826	14.984538
21.310959	968.127136	14.989555
21.385042	973.732046	14.994573
21.055598	977.118043	14.999591
21.052062	966.375855	15.004608
21.089535	972.275004	15.009626
21.077648	969.400802	15.014643
21.283715	972.766627	15.019661
21.242234	970.402028	15.024679
21.423609	962.703113	15.029696
20.983714	977.482121	15.034714
21.138187	966.210641	15.039731
21.024951	972.740231	15.044749
21.069020	972.472796	15.049767
21.399284	972.002467	15.054784
21.528967	974.692780	15.059802
21.495231	971.117500	15.064819
21.482224	964.201133	15.069837
21.432035	975.667716	15.074855
21.596050	964.610396	15.079872
21.305448	971.973258	15.084890
21.481522	962.738670	15.089907
21.703327	969.687565	15.094925
21.633499	982.843949	15.099943
21.741807	967.529884	15.104960
21.341841	970.285851	15.109978
21.660738	983.531012	15.114995
22.004521	993.198191	15.120013
21.760121	986.370521	15.125031
21.688907	959.528789	15.130048
21.752590	970.684399	15.135066
22.056605	976.021719	15.140083
21.863764	970.010288	15.145101
21.821800	968.694939	15.150119
22.034860	966.251186	15.155136
21.823987	960.291168	15.160154
21.876467	955.572529	15.165171
22.089797	948.572630	15.170189
21.791259	963.493960	15.175207
22.149005	954.875724	15.180224
21.925213	959.560309	15.185242
21.910928	960.958373	15.190259
21.793213	952.266117	15.195277
21.799034	964.024585	15.200295
22.074857	961.367694	15.205312
22.000759	956.755050	15.210330
21.966557	964.569920	15.215347
21.790668	970.666202	15.220365
21.610757	987.321776	15.225383
22.148412	980.076435	15.230400
22.009744	998.188123	15.235418
22.108239	990.247417	15.240435
22.097699	991.232674	15.245453
21.816248	993.182439	15.250471
22.259325	982.527699	15.255488
22.121778	991.925380	15.260506
22.458086	981.822156	15.265523
22.337354	983.283121	15.270541
22.279739	990.691662	15.275559
22.147142	991.472336	15.280576
22.227161	986.649526	15.285594
22.271223	990.059503	15.290611
22.389789	986.950713	15.295629
22.511107	987.325578	15.300647
22.462463	985.606625	15.305664
22.314525	997.989767	15.310682
22.346152	1001.584475	15.315699
22.986617	1015.259075	15.320717
22.497572	1007.226284	15.325735
22.599634	982.080557	15.330752
22.630251	989.278039	15.335770
22.486382	993.901764	15.340787
22.553879	1003.106450	15.345805
22.612922	1014.756542	15.350823
22.760132	1012.738237	15.355840
22.687602	1018.825296	15.360858
22.974268	1021.908112	15.365875
23.138326	1008.715402	15.370893
22.908524	990.450725	15.375911
23.148042	979.495455	15.380928
23.142321	980.354722	15.385946
22.577055	969.643343	15.390963
23.196545	976.029955	15.395981
22.864423	979.482535	15.400999
22.739033	971.574185	15.406016
22.876993	978.947974	15.411034
22.890453	982.321285	15.416051
23.028949	980.748110	15.421069
22.887799	980.454260	15.426087
23.252716	981.067124	15.431104
22.903371	978.241318	15.436122
23.016058	976.385814	15.441139
22.820723	975.426555	15.446157
22.985061	981.901920	15.451175
23.041756	979.089192	15.456192
23.171520	988.514652	15.461210
23.144498	1002.833209	15.466227
23.233520	1003.026422	15.471245
23.073442	1014.665948	15.476263
23.296342	1006.723924	15.481280
23.122625	1016.703964	15.486298
23.082679	1014.882390	15.491315
23.527893	1010.244368	15.496333
23.089905	1014.312494	15.501351
23.264043	1008.651289	15.506368
23.195607	1018.422173	15.511386
23.349893	1013.018575	15.516403
23.833684	1006.862020	15.521421
22.879032	1017.624888	15.526439
23.259915	1007.761108	15.531456
23.251257	1016.420954	15.536474
23.198319	1023.919284	15.541491
23.480857	1017.150405	15.546509
23.148717	1020.947078	15.551527
23.024657	1008.632359	15.556544
23.145009	1020.040029	15.561562
23.452311	1032.839138	15.566579
23.485484	1028.509880	15.571597
23.711678	1029.610660	15.576615
23.652021	1018.903318	15.581632
23.697847	1029.369828	15.586650
23.312135	1032.370287	15.591667
23.560038	1027.847212	15.596685
23.837198	1024.443266	15.601703
23.888091	1020.216191	15.606720
23.595348	1025.714938	15.611738
23.692512	1027.126835	15.616755
23.880821	1020.884562	15.621773
24.115910	1024.136935	15.626791
24.175723	1025.211723	15.631808
24.166407	1030.880856	15.636826
23.985315	1039.116528	15.641843
23.852888	1023.532045	15.646861
23.689318	1028.183451	15.651879
23.919858	1020.307868	15.656896
24.005119	1022.690991	15.661914
23.730387	1023.225527	15.666931
23.983929	1031.686854	15.671949
23.875891	1041.181642	15.676967
24.389331	1054.689916	15.681984
24.486077	1039.991451	15.687002
23.901205	1031.710745	15.692019
24.417252	1028.669590	15.697037
24.455900	1038.689674	15.702055
24.619245	1022.433799	15.707072
24.536522	1019.086689	15.712090
24.370861	1026.745412	15.717107
24.342723	1022.342453	15.722125
24.359499	1030.578427	15.727143
24.345162	1020.253723	15.732160
24.585380	1016.691729	15.737178
24.502771	1017.638137	15.742195
24.527824	1018.277358	15.747213
24.408366	1019.080267	15.752231
24.342260	1020.696751	15.757248
24.648324	1017.355342	15.762266
24.431394	1023.118689	15.767283
24.583592	1012.748304	15.772301
24.297463	1019.704952	15.777319
24.294987	1009.588913	15.782336
24.629605	1024.220428	15.787354
24.460915	1041.890306	15.792371
25.004660	1042.493640	15.797389
24.953015	1052.657025	15.802407
24.567651	1031.363839	15.807424
24.274852	1039.976262	15.812442
24.355362	1046.528131	15.817459
24.987632	1042.173682	15.822477
24.610984	1042.597541	15.827495
24.910887	1047.156068	15.832512
24.742490	1042.534998	15.837530
24.556465	1049.313672	15.842547
24.895672	1045.191994	15.847565
25.029059	1044.027517	15.852583
25.081587	1042.904381	15.857600
25.098908	1048.401399	15.862618
24.745996	1046.988717	15.867635
24.738355	1049.482892	15.872653
24.987787	1047.907876	15.877671
24.735939	1049.009863	15.882688
25.000444	1045.807608	15.887706
25.144093	1062.103791	15.892723
25.312263	1064.532245	15.897741
25.428299	1051.703737	15.902759
25.426304	1039.742390	15.907776
25.513827	1045.238805	15.912794
24.843891	1043.843973	15.917811
24.945504	1036.123191	15.922829
25.338522	1046.950318	15.927847
25.646960	1050.059848	15.932864
25.538051	1033.444333	15.937882
25.125845	1050.268355	15.942899
25.313202	1043.876235	15.947917
25.229080	1039.938430	15.952935
25.547862	1056.877631	15.957952
25.878346	1062.626332	15.962970
25.230971	1051.921798	15.967987
25.514892	1049.283236	15.973005
25.277433	1059.200238	15.978023
25.423150	1064.231135	15.983040
25.710947	1060.184105	15.988058
25.231184	1060.721491	15.993075
25.815894	1060.018877	15.998093
25.525964	1063.162531	16.003111
25.750525	1064.668688	16.008128
25.787257	1058.775108	16.013146
25.244668	1072.854701	16.018163
25.964641	1056.179863	16.023181
25.942240	1067.162402	16.028199
25.955639	1069.193270	16.033216
25.811613	1061.771801	16.038234
26.139854	1064.380435	16.043251
25.843010	1056.312643	16.048269
25.964876	1067.502388	16.053287
25.739610	1067.874803	16.058304
25.854980	1053.983055	16.063322
25.780715	1072.265262	16.068339
25.969441	1067.149633	16.073357
25.792228	1064.403179	16.078375
25.931373	1066.953757	16.083392
25.945390	1063.901239	16.088410
26.077998	1065.354120	16.093427
25.846078	1063.529290	16.098445
26.035013	1082.814347	16.103463
26.171599	1092.113549	16.108480
26.314019	1097.197363	16.113498
26.463263	1100.714353	16.118515
26.597578	1083.952607	16.123533
26.469784	1083.351830	16.128551
26.544851	1071.680443	16.133568
26.326643	1055.936121	16.138586
26.157151	1061.105428	16.143603
26.484681	1059.370240	16.148621
26.467765	1055.824044	16.153639
26.466773	1052.229938	16.158656
26.428849	1052.766995	16.163674
26.401399	1070.283995	16.168691
26.901571	1083.334665	16.173709
26.603564	1079.418093	16.178727
26.349889	1069.570372	16.183744
26.468873	1076.197376	16.188762
26.510634	1097.767373	16.193779
26.670893	1088.421947	16.198797
26.602334	1089.446739	16.203815
26.419604	1092.506115	16.208832
26.690290	1089.191414	16.213850
26.417969	1083.354510	16.218867
26.588574	1084.327102	16.223885
26.717486	1083.407056	16.228903
26.453737	1091.372988	16.233920
26.706614	1079.000522	16.238938
26.584121	1084.082530	16.243955
26.680265	1073.806817	16.248973
26.770299	1098.463202	16.253991
27.049737	1103.576297	16.259008
27.742143	1102.686563	16.264026
27.192848	1096.617573	16.269043
26.936285	1087.795876	16.274061
27.109321	1079.981752	16.279079
26.926849	1077.706228	16.284096
27.280339	1076.667109	16.289114
27.120741	1084.704371	16.294131
27.236363	1079.841780	16.299149
27.160839	1083.126308	16.304167
26.938622	1081.109718	16.309184
27.137314	1084.656311	16.314202
27.213269	1096.996947	16.319219
27.477142	1104.007045	16.324237
27.576253	1109.329917	16.329255
27.530201	1097.780531	16.334272
27.274228	1081.684968	16.339290
27.298576	1081.159782	16.344307
27.579613	1089.432736	16.349325
27.569588	1100.163651	16.354343
27.512351	1098.545318	16.359360
27.702010	1085.959307	16.364378
27.437430	1081.149040	16.369395
27.485206	1085.791845	16.374413
27.585467	1084.109640	16.379431
27.468276	1104.917805	16.384448
27.870355	1098.514911	16.389466
27.858686	1106.314311	16.394483
27.943885	1096.676201	16.399501
27.849254	1082.824318	16.404519
27.527660	1086.098412	16.409536
27.781671	1084.129734	16.414554
27.842115	1100.516898	16.419571
27.967872	1105.176323	16.424589
28.371287	1105.361967	16.429607
27.881652	1093.256527	16.434624
27.732480	1076.247252	16.439642
27.789789	1073.782030	16.444659
27.744161	1088.860808	16.449677
28.000419	1096.086329	16.454695
27.739731	1104.515525	16.459712
27.839366	1105.377432	16.464730
27.419497	1109.882331	16.469747
27.634520	1102.719490	16.474765
27.799723	1100.715910	16.479783
27.985013	1104.956042	16.484800
28.140649	1110.111292	16.489818
28.213012	1130.127499	16.494835
28.277047	1128.634353	16.499853
28.769589	1133.638946	16.504871
28.132045	1123.491772	16.509888
28.367007	1119.130651	16.514906
28.304397	1131.873381	16.519923
28.688565	1129.009551	16.524941
28.667089	1118.019056	16.529959
28.353258	1102.193279	16.534976
28.055270	1096.172438	16.539994
28.094984	1115.263354	16.545011
28.551440	1122.157716	16.550029
28.652350	1121.565917	16.555047
28.340991	1121.928180	16.560064
28.542152	1126.043253	16.565082
28.501160	1125.166298	16.570099
28.689271	1135.977025	16.575117
28.992932	1123.530370	16.580135
28.503286	1123.878061	16.585152
28.608999	1119.517476	16.590170
28.673993	1122.790949	16.595187
28.970958	1125.274856	16.600205
28.888121	1120.341966	16.605223
28.764828	1122.169105	16.610240
28.629378	1117.058320	16.615258
28.910675	1118.243681	16.620275
28.764182	1115.831095	16.625293
28.962599	1115.332596	16.630311
28.625254	1122.374539	16.635328
28.713695	1127.598793	16.640346
28.761117	1125.124571	16.645363
28.915106	1147.448471	16.650381
29.372516	1155.930438	16.655399
28.797041	1154.117997	16.660416
28.931710	1151.334057	16.665434
29.170036	1166.117868	16.670451
29.159084	1150.982814	16.675469
29.306674	1151.746629	16.680487
29.419447	1147.693125	16.685504
29.390169	1140.391196	16.690522
29.680611	1149.090958	16.695539
29.557266	1150.835040	16.700557
29.438668	1135.978446	16.705575
29.726290	1148.154946	16.710592
29.504203	1147.050897	16.715610
29.555648	1145.498418	16.720627
29.574467	1145.376496	16.725645
29.428079	1140.252948	16.730663
29.327472	1145.660082	16.735680
29.695934	1149.853362	16.740698
29.470604	1148.878980	16.745715
29.584409	1148.366144	16.750733
29.217026	1142.391420	16.755751
29.497880	1144.569345	16.760768
29.520932	1151.749258	16.765786
29.460771	1142.120228	16.770803
29.308676	1147.079996	16.775821
29.629639	1158.652576	16.780839
30.019845	1169.609779	16.785856
30.000163	1172.486666	16.790874
30.325079	1171.693604	16.795891
30.539103	1145.160609	16.800909
30.448444	1132.941831	16.805927
30.236925	1133.047807	16.810944
30.175967	1134.196142	16.815962
30.316089	1123.152507	16.820979
30.269984	1117.743079	16.825997
30.409783	1116.118889	16.831015
30.271467	1136.718791	16.836032
30.495841	1122.410519	16.841050
30.309696	1130.797859	16.846067
30.067116	1123.904867	16.851085
30.238249	1122.008961	16.856103
30.276268	1121.822051	16.861120
30.431399	1115.625389	16.866138
30.492231	1122.336450	16.871155
30.118946	1126.099411	16.876173
30.323052	1118.100207	16.881191
30.160492	1114.674174	16.886208
30.201394	1114.743077	16.891226
30.179727	1117.436823	16.896243
29.768109	1127.293733	16.901261
30.305614	1119.196806	16.906279
30.265390	1149.369942	16.911296
30.567568	1156.237899	16.916314
30.721120	1158.176676	16.921331
30.433023	1158.212657	16.926349
30.651313	1159.342314	16.931367
30.544908	1159.659224	16.936384
30.630733	1159.917928	16.941402
31.102161	1160.722213	16.946419
30.786847	1158.299781	16.951437
30.837987	1160.238981	16.956455
31.002596	1157.385518	16.961472
30.973351	1158.325854	16.966490
31.169740	1159.788655	16.971507
30.892947	1168.051658	16.976525
30.791812	1156.237736	16.981543
30.607401	1156.573861	16.986560
30.942410	1156.917285	16.991578
30.591658	1164.970492	16.996595
30.477156	1158.897198	17.001613
30.858578	1169.929476	17.006631
30.931857	1183.456418	17.011648
31.350652	1184.592245	17.016666
31.550806	1180.510092	17.021683
31.045245	1176.094805	17.026701
31.200057	1174.051600	17.031719
31.587465	1176.335111	17.036736
31.432582	1173.076292	17.041754
31.359489	1167.731944	17.046771
31.088811	1178.211986	17.051789
31.521582	1169.654436	17.056807
31.832060	1181.014208	17.061824
31.849553	1183.061342	17.066842
31.778184	1180.526862	17.071859
31.458141	1184.470386	17.076877
31.455046	1168.592695	17.081895
31.291228	1174.725639	17.086912
31.412538	1170.656937	17.091930
31.680534	1178.766355	17.096947
31.548586	1186.366426	17.101965
31.661930	1188.627211	17.106983
31.635172	1175.431704	17.112000
31.273602	1175.794015	17.117018
31.810591	1181.405027	17.122035
31.863808	1203.481134	17.127053
32.114506	1200.003582	17.132071
32.089501	1196.592154	17.137088
32.218257	1187.302671	17.142106
32.508204	1169.171400	17.147123
32.130048	1168.825454	17.152141
32.130825	1167.974256	17.157159
32.239784	1169.542477	17.162176
32.038170	1165.801648	17.167194
32.251299	1165.025522	17.172211
32.235759	1175.341667	17.177229
32.521119	1165.914458	17.182247
32.254945	1174.511130	17.187264
32.093932	1174.160331	17.192282
32.350028	1164.100191	17.197299
32.135084	1171.784469	17.202317
32.618905	1158.123736	17.207335
32.497102	1170.765673	17.212352
32.458122	1158.067860	17.217370
32.530930	1160.508969	17.222387
32.166533	1163.716153	17.227405
32.479098	1164.101088	17.232423
32.198577	1173.545779	17.237440
32.208958	1189.079541	17.242458
32.679121	1188.299042	17.247475
32.342851	1197.848646	17.252493
32.480220	1186.831799	17.257511
32.603913	1188.883003	17.262528
32.873943	1190.881629	17.267546
32.860815	1189.091027	17.272563
32.782244	1189.972605	17.277581
32.539574	1185.920861	17.282599
32.644778	1185.525586	17.287616
32.718876	1193.506887	17.292634
32.961079	1192.377923	17.297651
32.812139	1202.756725	17.302669
32.811409	1209.451639	17.307687
32.996662	1214.393758	17.312704
32.853842	1222.677126	17.317722
33.422316	1212.326655	17.322739
32.985059	1218.437965	17.327757
33.459672	1218.253563	17.332775
33.383986	1208.863277	17.337792
33.106644	1209.819893	17.342810
33.133563	1212.736707	17.347827
33.187519	1215.673454	17.352845
33.126772	1208.526700	17.357863
33.447087	1213.438581	17.362880
33.192426	1217.985444	17.367898
33.624984	1215.818293	17.372915
33.531221	1220.740080	17.377933
33.687562	1217.021462	17.382951
33.598598	1207.015281	17.387968
33.570120	1210.461333	17.392986
33.782486	1208.451505	17.398003
33.608250	1211.866181	17.403021
33.651740	1215.671174	17.408039
33.347232	1209.785616	17.413056
33.333103	1214.613115	17.418074
33.693177	1207.128972	17.423091
33.682417	1214.666078	17.428109
33.398583	1209.193228	17.433127
33.332427	1223.318081	17.438144
33.725278	1244.793536	17.443162
34.448505	1242.538095	17.448179
34.094323	1247.643953	17.453197
33.945231	1240.551575	17.458215
34.071247	1251.682106	17.463232
33.798995	1249.709605	17.468250
34.341333	1241.805511	17.473267
34.190983	1241.721835	17.478285
34.220421	1243.054418	17.483303
34.318395	1237.347869	17.488320
34.029724	1247.493938	17.493338
34.439680	1239.386180	17.498355
34.281872	1237.046707	17.503373
34.036504	1239.951134	17.508391
34.662897	1230.678829	17.513408
34.319651	1238.671778	17.518426
34.321433	1228.482845	17.523443
34.645844	1230.699632	17.528461
34.515983	1238.165135	17.533479
34.879445	1232.248884	17.538496
34.331054	1241.838757	17.543514
34.678983	1228.518173	17.548531
34.432720	1236.286012	17.553549
34.494097	1237.868024	17.558567
34.942302	1226.829207	17.563584
34.567656	1234.712396	17.568602
34.798785	1228.038550	17.573619
34.598967	1232.575549	17.578637
34.563937	1231.754293	17.583655
34.475783	1233.438621	17.588672
34.554329	1235.959106	17.593690
34.806794	1241.611740	17.598707
35.091345	1250.161358	17.603725
34.890204	1261.965345	17.608743
34.913731	1259.018297	17.613760
35.195501	1263.488949	17.618778
35.143930	1253.122618	17.623795
35.295643	1253.388129	17.628813
35.073156	1254.953367	17.633831
35.307309	1258.849239	17.638848
34.967210	1264.623227	17.643866
35.228980	1258.093111	17.648883
35.177532	1261.254401	17.653901
35.131211	1260.796028	17.658919
35.382836	1253.689260	17.663936
35.172473	1254.426132	17.668954
35.420915	1246.082128	17.673971
35.237407	1256.844633	17.678989
35.104212	1257.239995	17.684007
35.164904	1256.829256	17.689024
35.358580	1275.964954	17.694042
35.783453	1279.230052	17.699059
35.912958	1280.132692	17.704077
35.991327	1290.257383	17.709095
36.251553	1277.137890	17.714112
35.472769	1268.203350	17.719130
35.543628	1256.853379	17.724147
35.818578	1269.906069	17.729165
36.125809	1282.050689	17.734183
36.263299	1272.449479	17.739200
35.954039	1260.042786	17.744218
35.905280	1247.648087	17.749235
35.968599	1255.218221	17.754253
36.194932	1270.964333	17.759271
36.515763	1269.361726	17.764288
36.068806	1259.378174	17.769306
36.119215	1248.075690	17.774323
36.129943	1249.529873	17.779341
35.909778	1252.199818	17.784359
36.386379	1265.762016	17.789376
35.958928	1275.663372	17.794394
36.192759	1265.056866	17.799411
36.587738	1270.080809	17.804429
36.304773	1273.809559	17.809447
36.476760	1283.068370	17.814464
36.210851	1271.320224	17.819482
36.377844	1264.703044	17.824499
36.651040	1273.875407	17.829517
36.448408	1271.509100	17.834535
36.709193	1263.444533	17.839552
36.444585	1271.574081	17.844570
36.598102	1269.266516	17.849587
36.721500	1266.825360	17.854605
36.373213	1270.488155	17.859623
36.926959	1264.447867	17.864640
36.840116	1266.217807	17.869658
36.640676	1271.295688	17.874675
36.833887	1271.681097	17.879693
36.344487	1285.177677	17.884711
36.701081	1289.991452	17.889728
36.625007	1300.165344	17.894746
36.884318	1291.304172	17.899763
37.501698	1288.845784	17.904781
37.267562	1297.849809	17.909799
37.345025	1288.296717	17.914816
37.091336	1292.797773	17.919834
37.370958	1295.265288	17.924851
37.221750	1295.999123	17.929869
36.819543	1289.019498	17.934887
37.312359	1285.353415	17.939904
37.418621	1292.927481	17.944922
37.622786	1288.040715	17.949939
37.428523	1280.487697	17.954957
36.871670	1282.633882	17.959975
37.709564	1290.223020	17.964992
37.464809	1289.639238	17.970010
37.314031	1291.794562	17.975027
37.546218	1293.889231	17.980045
37.179475	1305.578942	17.985063
37.702231	1310.136081	17.990080
37.859099	1315.672291	17.995098
37.915413	1318.707090	18.000115
38.058511	1320.386601	18.005133
38.181045	1310.803198	18.010151
38.306248	1300.684331	18.015168
37.977719	1294.660594	18.020186
38.077916	1291.967375	18.025203
37.999989	1285.649791	18.030221
37.760296	1283.296704	18.035239
37.895761	1271.981694	18.040256
37.923762	1292.239309	18.045274
38.021289	1308.582366	18.050291
37.984683	1308.074746	18.055309
38.146451	1320.380093	18.060327
38.162955	1316.751533	18.065344
38.377763	1315.197972	18.070362
38.462650	1307.474312	18.075379
38.358403	1305.630675	18.080397
38.160227	1310.703241	18.085415
38.721899	1320.412894	18.090432
38.435890	1316.308843	18.095450
38.448743	1307.525478	18.100467
38.373113	1310.484881	18.105485
38.147528	1309.880995	18.110503
38.644229	1309.265385	18.115520
38.474127	1315.021086	18.120538
38.513183	1314.221809	18.125555
38.799478	1319.022430	18.130573
38.896632	1333.380574	18.135591
39.245370	1319.804665	18.140608
39.019558	1322.253514	18.145626
38.711944	1322.654530	18.150643
38.958044	1302.076867	18.155661
38.595976	1310.506819	18.160679
38.607731	1311.042351	18.165696
38.656422	1323.393982	18.170714
38.888729	1333.443607	18.175731
38.877343	1325.503207	18.180749
38.954534	1329.281782	18.185767
39.008031	1321.753073	18.190784
39.116432	1323.377307	18.195802
39.091850	1321.874801	18.200819
39.358918	1325.825080	18.205837
39.501564	1340.473330	18.210855
39.722141	1347.245044	18.215872
39.521334	1343.384354	18.220890
39.104116	1334.898165	18.225907
39.616631	1329.145384	18.230925
39.664663	1345.845488	18.235943
39.653469	1346.704501	18.240960
39.696625	1353.727638	18.245978
39.840862	1358.789192	18.250995
39.995255	1343.996249	18.256013
39.922465	1329.574002	18.261031
39.524628	1317.239015	18.266048
39.892458	1317.319534	18.271066
40.080070	1308.969821	18.276083
40.156203	1308.769511	18.281101
39.766503	1317.117823	18.286119
39.546958	1315.972002	18.291136
39.923567	1308.810656	18.296154
39.677340	1339.797392	18.301171
40.088460	1342.545106	18.306189
40.000952	1342.928968	18.311207
40.303425	1341.561673	18.316224
40.176529	1340.222166	18.321242
39.890123	1352.823003	18.326259
39.633272	1346.479115	18.331277
40.046621	1347.764675	18.336295
40.148128	1343.568106	18.341312
40.092253	1360.133071	18.346330
40.085192	1373.549074	18.351347
40.504838	1365.136108	18.356365
40.582757	1372.596798	18.361383
40.487970	1373.801145	18.366400
40.346657	1376.761988	18.371418
40.369516	1364.301793	18.376435
40.966700	1361.362888	18.381453
40.157843	1381.533600	18.386471
40.287507	1373.907216	18.391488
40.645730	1366.856761	18.396506
41.043430	1381.967535	18.401523
40.659342	1374.792354	18.406541
40.960149	1384.084618	18.411559
41.095447	1387.220918	18.416576
41.176607	1384.668235	18.421594
41.392358	1390.143542	18.426611
41.302863	1372.643751	18.431629
40.921722	1360.683912	18.436647
41.448801	1359.665245	18.441664
41.266260	1354.759026	18.446682
41.260076	1355.363277	18.451699
41.197120	1350.920321	18.456717
41.442095	1358.527749	18.461735
41.443378	1356.270969	18.466752
41.542946	1357.246286	18.471770
41.093074	1362.662902	18.476787
41.608606	1360.002867	18.481805
41.550752	1382.436986	18.486823
41.331510	1375.724659	18.491840
41.720733	1380.716916	18.496858
42.076831	1381.514328	18.501875
42.081004	1371.369785	18.506893
41.922994	1359.756459	18.511911
42.088796	1344.426596	18.516928
41.749399	1339.069197	18.521946
41.722499	1339.801679	18.526963
41.521651	1344.132979	18.531981
42.076462	1360.109040	18.536999
42.246390	1371.220577	18.542016
42.391137	1363.551150	18.547034
42.031182	1355.210977	18.552051
42.174241	1341.166751	18.557069
41.959669	1343.165719	18.562087
42.023987	1353.371911	18.567104
42.253588	1362.106278	18.572122
42.158897	1373.690365	18.577139
42.363730	1360.942172	18.582157
42.034431	1374.095789	18.587175
42.128914	1369.857464	18.592192
42.209124	1376.081182	18.597210
42.177532	1372.440494	18.602227
42.148533	1369.016697	18.607245
42.413285	1377.919659	18.612263
42.380807	1372.751582	18.617280
42.631905	1382.565848	18.622298
42.547983	1390.591525	18.627315
42.401417	1394.013077	18.632333
42.652669	1400.884458	18.637351
42.690277	1399.886994	18.642368
42.965344	1396.832130	18.647386
42.368702	1395.601106	18.652403
42.305617	1399.805282	18.657421
42.383404	1400.449961	18.662439
42.678931	1419.662279	18.667456
43.157213	1419.701282	18.672474
43.117602	1425.977537	18.677491
43.532928	1425.396657	18.682509
43.238809	1423.041537	18.687527
43.357346	1424.622372	18.692544
43.365182	1420.569637	18.697562
43.292121	1417.401154	18.702579
43.274369	1425.805258	18.707597
43.317154	1422.067598	18.712615
43.413351	1422.888755	18.717632
43.708451	1413.405061	18.722650
43.361914	1423.485236	18.727667
43.608054	1408.599089	18.732685
43.643922	1413.429001	18.737703
43.847117	1418.157588	18.742720
44.068001	1413.310927	18.747738
43.904344	1417.267197	18.752755
44.121815	1412.965583	18.757773
44.064167	1412.279949	18.762791
43.826177	1396.329108	18.767808
43.952969	1398.162901	18.772826
43.905270	1409.516008	18.777843
43.997143	1412.902020	18.782861
44.100629	1408.420071	18.787879
43.868884	1424.473681	18.792896
43.855521	1412.670619	18.797914
43.841594	1408.738418	18.802931
43.787748	1413.776884	18.807949
44.158323	1412.104216	18.812967
44.120317	1419.297513	18.817984
44.261593	1414.496316	18.823002
44.045014	1420.806988	18.828019
44.540678	1428.965849	18.833037
44.432093	1435.283842	18.838055
44.433105	1448.748574	18.843072
44.897267	1438.769553	18.848090
44.543829	1445.587536	18.853107
44.855443	1428.788581	18.858125
44.820528	1438.474258	18.863143
44.673778	1439.779339	18.868160
44.597147	1432.609521	18.873178
44.750141	1437.167688	18.878195
44.807114	1438.250455	18.883213
44.966488	1441.753249	18.888231
44.638528	1440.111202	18.893248
44.990767	1437.674647	18.898266
44.763498	1439.129672	18.903283
45.015156	1438.214085	18.908301
45.244539	1434.047106	18.913319
45.226896	1439.413439	18.918336
45.214824	1431.714827	18.923354
44.801611	1431.971521	18.928371
45.242982	1438.983091	18.933389
45.407039	1440.654421	18.938407
45.515374	1454.186425	18.943424
45.720981	1442.824637	18.948442
45.457157	1432.679942	18.953459
45.570390	1429.061323	18.958477
45.298399	1428.579288	18.963495
45.082044	1455.124747	18.968512
45.251073	1441.926122	18.973530
45.451372	1461.252291	18.978547
45.495078	1454.686546	18.983565
45.726396	1461.145512	18.988583
45.700498	1455.573959	18.993600
45.784179	1460.049910	18.998618
45.843171	1456.000900	19.003635
45.895593	1456.643089	19.008653
45.823087	1451.994207	19.013671
46.025917	1474.504192	19.018688
46.601202	1474.632645	19.023706
46.262060	1478.125865	19.028723
46.196404	1457.038204	19.033741
46.309602	1456.664041	19.038759
45.913810	1458.271773	19.043776
46.380749	1462.911429	19.048794
46.184166	1474.489234	19.053811
46.245895	1475.064135	19.058829
46.462274	1479.599221	19.063847
46.282883	1480.119165	19.068864
46.517595	1470.273391	19.073882
46.600207	1475.412115	19.078899
46.758293	1478.317891	19.083917
46.740520	1469.686354	19.088935
46.441975	1480.887350	19.093952
46.897598	1472.053413	19.098970
46.523086	1474.430451	19.103987
46.767120	1476.457830	19.109005
47.079223	1480.295577	19.114023
46.872538	1492.025066	19.119040
47.394836	1493.174884	19.124058
46.966445	1493.295116	19.129075
46.812510	1496.232874	19.134093
47.324580	1496.133608	19.139111
47.221959	1500.110894	19.144128
47.396318	1494.947898	19.149146
47.362996	1502.379826	19.154163
47.345346	1500.580488	19.159181
47.196162	1497.435222	19.164199
47.248768	1500.830511	19.169216
47.486942	1502.487213	19.174234
47.861441	1497.593044	19.179251
47.490722	1503.789903	19.184269
47.786799	1493.632381	19.189287
47.564034	1494.158720	19.194304
47.868384	1489.808448	19.199322
47.805016	1490.133199	19.204339
47.538091	1495.846337	19.209357
47.763941	1489.063019	19.214375
47.417600	1495.484970	19.219392
47.496300	1483.267794	19.224410
47.883956	1504.052352	19.229427
48.184213	1513.718800	19.234445
48.458022	1512.422378	19.239463
48.283199	1519.575777	19.244480
48.229861	1520.810673	19.249498
48.459740	1512.390074	19.254515
48.521054	1511.841430	19.259533
48.374014	1506.244249	19.264551
48.269650	1520.678059	19.269568
48.609942	1514.024599	19.274586
48.552354	1516.117280	19.279603
48.464808	1509.534269	19.284621
48.570829	1503.768417	19.289639
48.496067	1507.319441	19.294656
48.500507	1513.677019	19.299674
48.672570	1508.486447	19.304691
48.656714	1507.477356	19.309709
49.013766	1508.126980	19.314727
48.668610	1509.560981	19.319744
48.766061	1503.861114	19.324762
48.868511	1510.204430	19.329779
48.892590	1510.250925	19.334797
48.971691	1496.309668	19.339815
49.149480	1504.134985	19.344832
49.063307	1509.346549	19.349850
48.991886	1502.254182	19.354867
48.936157	1510.620132	19.359885
49.177985	1512.965202	19.364903
49.310841	1538.789602	19.369920
49.306479	1539.663242	19.374938
49.439948	1544.943175	19.379955
49.632851	1548.051072	19.384973
49.653536	1535.057638	19.389991
50.020249	1533.195048	19.395008
49.721814	1534.172891	19.400026
49.789290	1531.465364	19.405043
49.771749	1540.824215	19.410061
50.152745	1532.152993	19.415079
49.819055	1532.159908	19.420096
49.615439	1534.450391	19.425114
49.886517	1522.941878	19.430131
49.619842	1530.981352	19.435149
49.802255	1530.844544	19.440167
49.795800	1537.122440	19.445184
49.815942	1531.810952	19.450202
49.937134	1520.922531	19.455219
49.818849	1534.595671	19.460237
50.169873	1540.874221	19.465255
49.950119	1562.831473	19.470272
49.773933	1554.501314	19.475290
50.260971	1556.936105	19.480307
49.931038	1566.719135	19.485325
50.211167	1567.814176	19.490343
50.615415	1576.866202	19.495360
50.479420	1582.921078	19.500378
50.638475	1588.830252	19.505395
51.046303	1584.804946	19.510413
50.747409	1583.444684	19.515431
50.762006	1580.791967	19.520448
51.008893	1584.566522	19.525466
51.341245	1573.046645	19.530483
50.972024	1580.471236	19.535501
51.309948	1577.734669	19.540519
51.230204	1573.043248	19.545536
51.470527	1576.716133	19.550554
51.673180	1573.826767	19.555571
51.123263	1559.650235	19.560589
51.212337	1549.101363	19.565607
51.280492	1561.156262	19.570624
51.416629	1561.438138	19.575642
51.566428	1573.397639	19.580659
51.547270	1571.489881	19.585677
51.473207	1573.503014	19.590695
51.154098	1570.710671	19.595712
51.403495	1574.990319	19.600730
51.596503	1576.826161	19.605747
51.349985	1574.098963	19.610765
51.725147	1560.236974	19.615783
51.310060	1578.302196	19.620800
51.675291	1582.836288	19.625818
51.958575	1599.092596	19.630835
51.729406	1601.498344	19.635853
52.143753	1588.714880	19.640871
52.006618	1589.637673	19.645888
52.316325	1595.045528	19.650906
52.502741	1596.504511	19.655923
52.058326	1600.149047	19.660941
52.071046	1594.279318	19.665959
51.998779	1596.442156	19.670976
51.955559	1602.123017	19.675994
51.960291	1593.204614	19.681011
51.852159	1597.554097	19.686029
52.059561	1606.130467	19.691047
52.330434	1630.185711	19.696064
52.596933	1626.099937	19.701082
52.751184	1628.604014	19.706099
52.448946	1624.808867	19.711117
52.572520	1628.178654	19.716135
52.708463	1623.173158	19.721152
52.588306	1624.367945	19.726170
52.668301	1628.054397	19.731187
52.934679	1640.898978	19.736205
53.300089	1640.543287	19.741223
53.154993	1639.331570	19.746240
53.409633	1632.799722	19.751258
53.639886	1635.625075	19.756275
53.467690	1639.428484	19.761293
53.778543	1634.332212	19.766311
53.437562	1623.203708	19.771328
53.032187	1624.633122	19.776346
53.372692	1632.505972	19.781363
53.337974	1635.034252	19.786381
53.678946	1638.053085	19.791399
53.664744	1641.394112	19.796416
53.660419	1637.745697	19.801434
53.758256	1633.061075	19.806451
53.559327	1642.437029	19.811469
53.771807	1638.538543	19.816487
53.867553	1632.397178	19.821504
53.355941	1632.423315	19.826522
53.751154	1637.472539	19.831539
53.815390	1656.902190	19.836557
54.121581	1664.294122	19.841575
54.181575	1662.239781	19.846592
54.179758	1656.545272	19.851610
54.637037	1660.226349	19.856627
54.323765	1661.660201	19.861645
54.468070	1651.484792	19.866663
54.615440	1657.559314	19.871680
54.537683	1659.105352	19.876698
54.615220	1646.580759	19.881715
54.550138	1655.239281	19.886733
54.395862	1656.132239	19.891751
54.404297	1649.260047	19.896768
54.579372	1657.855971	19.901786
54.724233	1652.581272	19.906803
54.719010	1655.716091	19.911821
54.719971	1665.271167	19.916839
54.662480	1676.943021	19.921856
54.579586	1687.389164	19.926874
55.008175	1680.471800	19.931891
54.863450	1680.927742	19.936909
55.008234	1685.019624	19.941927
55.055751	1676.670076	19.946944
55.374469	1695.867481	19.951962
55.686594	1701.450171	19.956979
55.418326	1702.000980	19.961997
55.549520	1689.363137	19.967015
55.408064	1684.387410	19.972032
55.484128	1697.062368	19.977050
55.914141	1695.964873	19.982067
55.987401	1695.502828	19.987085
56.018480	1681.435498	19.992103
56.019302	1673.976364	19.997120
55.806900	1673.139176	20.002138
55.800902	1659.903204	20.007155
55.831806	1664.922206	20.012173
55.972565	1667.457658	20.017191
55.994872	1690.287612	20.022208
55.887156	1694.639809	20.027226
56.144107	1696.734765	20.032243
56.190105	1694.673683	20.037261
56.388057	1693.174845	20.042279
56.598478	1686.499115	20.047296
56.698137	1692.453597	20.052314
56.644465	1692.916117	20.057331
56.266680	1692.724425	20.062349
56.576809	1686.977466	20.067367
56.907943	1685.614058	20.072384
56.691201	1688.798473	20.077402
56.891248	1681.573279	20.082419
56.568772	1692.800042	20.087437
56.326128	1688.658396	20.092455
56.520714	1688.908943	20.097472
56.519582	1688.556067	20.102490
56.903262	1697.215900	20.107507
56.804858	1715.210341	20.112525
56.923474	1711.263598	20.117543
57.295127	1706.565507	20.122560
57.309500	1711.111668	20.127578
57.486588	1702.307185	20.132595
57.401353	1712.471447	20.137613
57.743034	1705.815314	20.142631
57.341669	1706.098001	20.147648
57.476141	1712.579013	20.152666
57.214296	1700.363327	20.157683
57.220778	1710.326574	20.162701
56.952744	1713.072240	20.167719
57.477518	1719.608316	20.172736
57.685339	1736.173722	20.177754
57.986802	1725.220270	20.182771
57.976181	1720.105939	20.187789
57.845574	1730.428513	20.192807
58.137122	1728.277556	20.197824
58.021870	1735.114495	20.202842
58.287444	1723.351626	20.207859
58.306315	1733.204567	20.212877
58.174119	1725.359950	20.217895
58.218804	1727.203833	20.222912
58.401793	1726.686611	20.227930
58.570298	1725.944227	20.232947
58.442525	1728.304858	20.237965
58.562429	1729.107933	20.242983
58.813569	1734.748371	20.248000
58.497560	1742.232338	20.253018
58.637228	1742.755762	20.258035
58.899064	1749.736965	20.263053
58.699050	1750.063480	20.268071
59.124503	1750.943132	20.273088
59.050206	1747.243678	20.278106
59.167674	1740.413236	20.283123
59.081267	1737.676821	20.288141
59.012091	1735.789922	20.293159
59.384286	1735.221687	20.298176
59.407721	1738.797056	20.303194
59.669396	1727.841135	20.308211
59.492122	1738.849006	20.313229
59.348904	1736.698774	20.318247
59.684995	1735.009342	20.323264
59.922645	1729.989334	20.328282
59.816513	1735.607432	20.333299
59.631235	1738.644520	20.338317
59.470958	1739.691627	20.343335
60.020257	1739.864152	20.348352
59.603640	1737.089498	20.353370
59.721317	1736.801595	20.358387
59.828320	1739.924936	20.363405
59.602354	1745.277443	20.368423
60.240850	1734.078021	20.373440
59.863007	1746.563606	20.378458
60.240592	1739.585370	20.383475
59.798587	1742.578745	20.388493
59.966774	1751.891224	20.393511
59.957362	1762.807931	20.398528
60.045034	1770.817598	20.403546
60.285630	1761.654925	20.408563
60.655812	1766.533925	20.413581
60.301014	1761.805310	20.418599
60.385277	1765.569829	20.423616
60.398566	1779.575341	20.428634
60.542259	1787.559598	20.433651
60.828891	1798.925351	20.438669
60.975593	1799.958248	20.443687
61.365313	1793.739405	20.448704
60.739138	1802.226736	20.453722
60.964006	1789.779996	20.458739
60.646320	1793.896511	20.463757
60.793916	1798.201345	20.468775
61.266487	1804.739016	20.473792
61.128167	1827.064658	20.478810
61.043415	1829.316605	20.483827
61.484674	1824.599473	20.488845
61.684392	1829.365771	20.493863
61.973381	1823.922660	20.498880
61.863195	1824.515409	20.503898
62.076842	1829.869961	20.508915
62.153226	1814.789876	20.513933
61.940950	1831.455257	20.518951
62.215468	1814.923449	20.523968
61.912342	1808.140175	20.528986
61.845166	1816.619997	20.534003
61.986634	1809.155621	20.539021
61.848082	1816.838984	20.544039
61.926240	1813.106792	20.549056
62.183943	1818.063488	20.554074
62.141515	1814.725675	20.559091
62.464788	1810.931638	20.564109
61.852459	1810.557122	20.569127
62.154621	1822.958523	20.574144
62.491060	1837.816893	20.579162
62.475051	1852.987968	20.584179
62.882788	1844.836171	20.589197
62.366096	1846.776956	20.594215
62.785215	1842.432781	20.599232
62.899105	1841.825027	20.604250
62.535273	1838.175853	20.609267
62.907676	1837.782386	20.614285
62.703296	1846.631011	20.619303
62.877465	1858.687092	20.624320
62.750943	1867.441734	20.629338
63.209779	1862.737429	20.634355
63.071889	1864.151315	20.639373
63.283025	1865.178666	20.644391
63.499483	1848.891084	20.649408
63.588835	1851.646892	20.654426
63.619290	1848.893864	20.659443
63.514237	1852.394076	20.664461
63.424318	1847.001490	20.669479
63.704469	1850.647374	20.674496
63.787009	1854.155109	20.679514
63.846550	1857.098928	20.684531
63.898952	1863.202641	20.689549
64.007228	1872.856220	20.694567
64.303669	1865.220879	20.699584
64.343589	1866.311225	20.704602
64.654929	1870.396446	20.709619
64.608733	1851.073166	20.714637
64.407777	1853.134904	20.719655
64.598785	1850.366316	20.724672
64.298316	1839.233310	20.729690
64.154319	1845.752611	20.734707
64.153282	1847.489511	20.739725
64.198092	1860.950105	20.744743
64.242026	1870.314331	20.749760
64.662334	1873.907092	20.754778
64.377694	1878.028787	20.759795
64.887339	1869.719550	20.764813
64.683854	1876.889276	20.769831
64.913899	1890.739705	20.774848
65.156155	1902.999119	20.779866
65.078574	1903.154968	20.784883
65.446864	1903.898028	20.789901
65.410875	1903.561943	20.794919
65.439076	1896.729282	20.799936
65.326761	1898.470439	20.804954
65.450888	1912.818749	20.809971
65.564529	1901.584848	20.814989
65.432529	1899.815026	20.820007
65.702450	1889.457243	20.825024
65.327081	1893.230179	20.830042
65.414069	1893.030427	20.835059
65.724161	1894.383528	20.840077
65.654450	1923.927610	20.845095
65.960596	1923.603774	20.850112
65.651315	1918.482134	20.855130
65.830150	1924.749587	20.860147
66.234685	1909.178061	20.865165
66.253115	1925.923063	20.870183
66.135088	1926.428135	20.875200
66.327936	1918.961893	20.880218
66.184435	1930.788733	20.885235
66.506112	1934.210828	20.890253
66.500685	1955.837473	20.895271
66.893354	1948.838536	20.900288
66.762582	1949.033902	20.905306
66.795323	1954.462939	20.910323
67.167582	1947.602424	20.915341
67.189064	1938.029067	20.920359
67.245160	1943.003830	20.925376
67.051289	1938.314658	20.930394
67.382270	1935.776428	20.935411
67.502859	1934.434475	20.940429
67.144023	1935.801484	20.945447
67.284922	1935.428235	20.950464
67.639437	1940.460282	20.955482
67.365412	1943.485332	20.960499
67.548118	1941.976397	20.965517
67.479807	1943.079551	20.970535
67.397587	1931.759551	20.975552
67.333879	1938.330166	20.980570
67.481602	1937.347900	20.985587
67.560061	1934.917624	20.990605
67.624872	1930.994696	20.995623
67.662818	1957.250084	21.000640
67.908313	1953.120852	21.005658
67.827640	1957.801722	21.010675
68.145877	1954.954962	21.015693
68.191823	1960.315278	21.020711
67.797581	1952.002111	21.025728
68.019582	1959.703801	21.030746
68.111949	1965.233208	21.035763
68.221838	1979.943394	21.040781
67.967541	1983.700636	21.045799
68.476217	1985.331108	21.050816
68.407646	1982.521223	21.055834
68.491239	1984.276803	21.060851
68.661668	1996.904885	21.065869
68.574047	1998.711651	21.070887
68.886032	2013.476599	21.075904
68.922018	2013.032528	21.080922
69.319141	2010.297897	21.085939
69.612735	2005.076408	21.090957
69.399756	2011.149314	21.095975
69.505234	2006.385360	21.100992
69.502710	1995.858831	21.106010
69.249518	2012.136682	21.111027
69.526559	1994.668809	21.116045
69.290319	2004.722040	21.121063
69.583748	2003.578241	21.126080
70.049052	1995.641249	21.131098
69.768090	1996.569374	21.136115
70.275665	1999.557545	21.141133
69.775045	1998.965308	21.146151
70.035903	1996.607581	21.151168
70.076190	1998.259701	21.156186
70.012320	2004.437447	21.161203
69.843634	2005.926919	21.166221
70.103824	2010.643102	21.171239
70.477539	2022.165078	21.176256
70.444991	2030.173130	21.181274
70.485523	2036.080840	21.186291
70.553019	2025.539548	21.191309
70.300950	2032.775265	21.196327
70.460092	2028.850473	21.201344
70.783343	2019.691287	21.206362
70.660770	2033.938820	21.211379
71.204189	2027.125917	21.216397
71.045378	2017.957963	21.221415
71.007338	2028.863456	21.226432
71.114733	2038.105067	21.231450
70.893817	2051.573602	21.236467
71.436677	2048.638845	21.241485
71.040975	2051.458465	21.246503
71.293429	2050.671850	21.251520
71.463501	2045.500328	21.256538
71.472890	2048.030428	21.261555
71.800765	2044.309985	21.266573
71.538144	2045.359489	21.271591
71.709719	2043.175991	21.276608
71.747730	2045.724974	21.281626
71.561036	2071.785853	21.286643
71.921259	2065.790297	21.291661
71.963733	2071.309105	21.296679
71.895091	2068.285430	21.301696
72.214284	2076.284481	21.306714
72.035088	2071.204244	21.311731
72.100372	2064.972475	21.316749
72.414515	2072.488881	21.321767
72.392220	2069.906758	21.326784
72.707348	2080.556956	21.331802
72.436525	2095.626753	21.336819
72.492455	2094.476206	21.341837
72.832183	2089.866755	21.346855
72.480964	2081.750337	21.351872
72.770478	2079.846921	21.356890
73.155521	2090.006402	21.361907
72.860107	2084.270974	21.366925
73.149514	2080.297828	21.371943
73.092234	2081.752326	21.376960
73.226997	2082.546660	21.381978
73.109533	2083.628434	21.386995
73.676394	2081.824771	21.392013
73.513545	2084.993256	21.397031
73.641811	2085.105182	21.402048
73.648154	2078.530792	21.407066
73.476135	2097.986334	21.412083
73.864325	2104.177069	21.417101
73.689347	2112.961526	21.422119
73.905885	2109.970942	21.427136
74.076922	2116.103145	21.432154
74.020536	2128.485415	21.437171
74.487152	2114.749530	21.442189
74.681948	2115.671726	21.447207
74.478489	2123.102199	21.452224
74.635983	2111.632138	21.457242
74.548057	2121.075436	21.462259
74.383160	2116.816072	21.467277
74.859412	2103.159707	21.472295
74.222182	2108.542241	21.477312
74.578056	2107.868819	21.482330
74.376789	2115.646968	21.487347
74.327110	2111.805157	21.492365
74.473599	2120.996250	21.497383
74.516883	2130.870206	21.502400
75.065589	2125.476905	21.507418
74.795237	2136.954814	21.512435
75.075709	2134.243020	21.517453
75.007045	2141.299596	21.522471
74.845874	2163.776361	21.527488
75.175958	2163.419030	21.532506
75.432262	2169.409573	21.537523
75.630885	2173.786775	21.542541
75.798838	2163.218914	21.547559
75.734462	2166.490407	21.552576
75.876330	2154.769743	21.557594
75.657224	2166.604556	21.562611
76.027422	2169.277305	21.567629
76.177114	2180.476636	21.572647
76.317481	2183.791007	21.577664
76.487724	2174.700766	21.582682
75.952030	2177.772728	21.587699
76.181936	2188.188677	21.592717
76.325203	2181.049428	21.597735
76.444272	2183.932270	21.602752
76.512684	2169.773273	21.607770
76.470832	2184.219791	21.612787
76.671048	2179.005831	21.617805
76.642818	2194.348954	21.622823
76.935824	2205.190703	21.627840
77.427626	2199.886330	21.632858
77.174119	2212.157204	21.637875
77.247857	2199.181597	21.642893
77.379327	2203.694341	21.647911
77.126412	2208.847522	21.652928
77.701121	2198.204810	21.657946
77.588985	2208.914816	21.662963
77.345344	2199.856472	21.667981
77.346335	2199.637096	21.672999
77.373248	2201.935177	21.678016
77.534773	2193.293630	21.683034
77.412729	2200.990198	21.688051
77.721775	2199.176058	21.693069
77.905751	2219.049204	21.698087
77.887899	2223.133903	21.703104
78.053898	2227.652748	21.708122
78.075039	2231.041596	21.713139
78.154912	2223.444695	21.718157
78.161587	2224.024803	21.723175
77.944812	2226.262838	21.728192
78.587291	2222.850121	21.733210
78.309872	2231.789406	21.738227
78.733132	2241.170974	21.743245
78.817857	2251.746836	21.748263
78.734859	2252.922918	21.753280
78.961245	2249.059382	21.758298
79.184836	2253.895878	21.763315
79.258197	2249.945862	21.768333
79.317231	2255.900595	21.773351
79.183115	2258.435984	21.778368
79.399323	2241.917709	21.783386
79.519536	2248.974559	21.788403
79.376393	2240.462174	21.793421
79.670635	2242.898684	21.798439
79.432081	2248.620390	21.803456
79.421369	2242.204274	21.808474
79.515413	2248.072888	21.813491
79.489493	2245.398418	21.818509
79.411570	2261.376632	21.823527
79.645200	2264.882674	21.828544
79.809615	2268.614753	21.833562
80.038888	2269.789923	21.838579
80.104229	2269.059477	21.843597
80.417159	2283.860749	21.848615
80.410321	2296.620005	21.853632
80.758012	2293.849021	21.858650
80.801314	2298.116143	21.863667
80.725598	2287.939345	21.868685
80.940954	2288.188828	21.873703
80.872531	2299.502314	21.878720
81.197419	2287.414619	21.883738
80.899237	2293.507647	21.888755
81.013667	2284.761638	21.893773
81.299697	2284.490342	21.898791
80.973981	2290.506822	21.903808
81.004211	2286.664337	21.908826
81.468871	2283.259394	21.913843
81.234943	2284.041552	21.918861
81.427035	2280.936475	21.923879
81.659745	2289.988584	21.928896
82.006298	2293.093242	21.933914
81.800053	2303.136580	21.938931
81.776796	2304.082686	21.943949
81.916826	2297.547884	21.948967
82.026821	2303.496953	21.953984
82.034011	2303.616722	21.959002
81.999703	2292.592476	21.964019
82.186330	2300.800610	21.969037
81.912896	2289.174592	21.974055
81.914564	2315.049172	21.979072
82.205272	2321.410474	21.984090
82.711866	2328.334092	21.989107
82.189346	2332.153149	21.994125
82.519667	2329.544097	21.999143
82.145231	2333.283122	22.004160
82.772638	2343.638479	22.009178
83.209676	2352.102831	22.014195
83.200169	2348.646849	22.019213
83.232975	2340.104489	22.024231
83.072150	2349.922611	22.029248
83.629058	2345.702737	22.034266
83.393559	2348.860468	22.039283
83.193966	2352.811111	22.044301
83.589660	2349.581754	22.049319
83.565298	2343.587167	22.054336
83.479966	2340.001215	22.059354
83.356708	2339.640590	22.064371
83.539761	2349.914398	22.069389
83.756463	2364.402137	22.074407
83.617259	2378.151532	22.079424
83.622669	2370.279473	22.084442
83.791290	2376.419267	22.089459
83.797559	2392.769522	22.094477
84.215205	2399.671677	22.099495
84.600581	2402.507318	22.104512
84.621849	2390.069400	22.109530
84.751395	2393.200559	22.114547
84.461481	2403.347977	22.119565
84.735824	2394.790007	22.124583
85.092689	2396.637010	22.129600
84.831910	2390.716196	22.134618
84.896906	2401.678910	22.139635
85.247251	2418.669503	22.144653
85.475380	2418.398737	22.149671
85.553517	2423.008962	22.154688
85.517123	2426.790864	22.159706
85.562516	2412.098028	22.164723
85.675167	2422.802461	22.169741
85.898228	2410.429546	22.174759
85.811849	2417.043094	22.179776
85.885106	2417.721246	22.184794
85.812010	2412.504033	22.189811
85.735495	2414.540121	22.194829
86.024721	2411.830374	22.199847
85.924688	2411.213921	22.204864
86.113215	2403.467440	22.209882
86.134601	2425.948611	22.214899
86.131554	2433.920488	22.219917
86.273971	2431.749245	22.224935
86.666764	2438.190548	22.229952
86.456851	2431.449442	22.234970
86.556018	2437.059786	22.239987
86.797606	2455.324005	22.245005
87.341662	2466.766927	22.250023
87.415349	2463.126269	22.255040
87.437793	2462.626944	22.260058
87.398151	2447.718615	22.265075
87.241359	2461.152081	22.270093
87.498815	2449.633330	22.275111
87.359313	2462.552883	22.280128
87.304253	2460.476934	22.285146
87.577526	2457.215854	22.290163
87.509631	2460.069857	22.295181
87.738882	2454.274195	22.300199
87.669698	2460.676636	22.305216
87.787810	2467.096103	22.310234
88.145684	2473.486900	22.315251
87.809317	2483.975544	22.320269
88.329119	2480.803570	22.325287
88.409274	2475.977914	22.330304
88.173375	2470.797873	22.335322
88.230222	2462.043974	22.340339
88.064930	2485.643600	22.345357
88.368486	2491.698891	22.350375
88.796323	2500.406594	22.355392
88.775278	2505.657710	22.360410
89.151016	2495.672974	22.365427
89.049967	2499.304171	22.370445
88.996909	2505.200388	22.375463
89.096192	2499.312049	22.380480
89.047248	2499.773022	22.385498
89.569297	2494.956878	22.390515
89.242302	2502.249707	22.395533
89.496420	2514.935620	22.400551
89.628644	2526.775532	22.405568
89.544574	2529.089280	22.410586
89.894834	2521.656140	22.415603
89.743920	2519.958673	22.420621
90.134883	2531.737639	22.425639
89.760337	2523.492952	22.430656
89.580768	2524.851195	22.435674
90.234873	2531.809148	22.440691
90.117127	2547.019005	22.445709
90.237553	2559.027834	22.450727
90.261679	2557.098220	22.455744
90.391239	2550.163840	22.460762
90.481775	2548.434662	22.465779
90.475720	2559.689189	22.470797
90.890418	2567.892775	22.475815
90.719695	2573.235236	22.480832
90.843645	2590.435166	22.485850
90.996613	2578.186723	22.490867
90.756851	2576.940207	22.495885
91.076730	2598.950921	22.500903
91.564656	2600.858539	22.505920
91.534811	2607.636441	22.510938
91.914396	2602.361538	22.515955
91.767883	2610.902570	22.520973
91.997295	2602.161363	22.525991
91.993748	2594.619040	22.531008
92.140394	2607.903568	22.536026
92.397160	2598.716860	22.541043
92.382532	2595.839267	22.546061
92.087983	2592.251672	22.551079
92.343445	2589.826637	22.556096
92.493305	2596.964569	22.561114
92.519547	2588.797987	22.566131
92.832135	2613.086843	22.571149
92.947219	2606.232005	22.576167
92.689684	2611.809733	22.581184
92.515282	2605.334736	22.586202
92.859407	2621.085558	22.591219
92.822656	2617.429289	22.596237
92.917063	2613.665472	22.601255
92.992035	2621.800918	22.606272
93.048151	2640.320486	22.611290
93.256504	2650.246581	22.616307
93.524120	2653.658497	22.621325
93.643002	2642.007419	22.626343
93.984764	2644.112483	22.631360
93.890545	2643.932488	22.636378
94.205137	2638.069082	22.641395
94.359249	2641.000936	22.646413
94.085251	2640.250667	22.651431
94.298247	2640.432040	22.656448
94.395235	2650.627377	22.661466
94.476421	2651.582592	22.666483
94.481226	2667.919204	22.671501
94.452391	2662.638669	22.676519
94.614645	2665.518388	22.681536
94.417154	2673.284770	22.686554
94.488021	2658.126824	22.691571
94.564834	2671.291463	22.696589
94.520960	2682.096010	22.701607
94.797063	2685.891988	22.706624
94.631009	2688.142163	22.711642
95.272989	2689.093120	22.716659
95.300202	2692.218053	22.721677
95.255248	2707.848722	22.726695
95.825219	2706.391354	22.731712
95.819191	2720.954493	22.736730
95.787331	2719.777882	22.741747
95.942693	2720.499939	22.746765
95.766635	2722.749412	22.751783
95.924056	2717.639610	22.756800
95.944930	2716.171178	22.761818
96.108469	2710.406381	22.766835
96.084080	2717.373205	22.771853
96.035479	2735.816517	22.776871
96.735111	2743.072169	22.781888
96.262454	2742.906007	22.786906
96.674797	2735.076633	22.791923
96.658515	2738.215076	22.796941
96.741672	2744.641627	22.801959
96.902269	2752.588542	22.806976
97.096700	2769.258064	22.811994
96.996007	2764.206731	22.817011
97.279407	2767.164057	22.822029
97.310759	2758.435475	22.827047
97.664859	2758.609236	22.832064
97.320063	2766.206731	22.837082
97.797934	2770.293757	22.842099
97.858932	2783.332753	22.847117
97.649349	2785.802370	22.852135
98.138657	2784.846182	22.857152
98.431671	2788.715375	22.862170
98.488048	2781.793403	22.867187
98.313415	2782.040925	22.872205
98.375508	2780.818043	22.877223
98.610252	2773.582663	22.882240
98.470273	2776.841995	22.887258
98.496909	2776.854210	22.892275
99.044115	2795.386757	22.897293
98.961588	2804.609085	22.902311
99.284459	2803.285934	22.907328
99.022813	2807.897802	22.912346
99.409693	2795.423832	22.917363
99.344113	2804.335457	22.922381
99.507656	2807.024817	22.927399
99.722157	2791.376784	22.932416
99.260651	2802.063537	22.937434
99.633884	2795.109967	22.942451
99.574821	2802.443620	22.947469
99.822313	2819.448926	22.952487
100.096257	2823.180329	22.957504
99.968828	2831.353726	22.962522
99.958336	2826.038206	22.967539
100.206143	2827.411943	22.972557
100.294638	2827.187914	22.977575
100.547175	2823.949091	22.982592
100.670820	2833.167224	22.987610
100.814543	2842.595835	22.992627
101.114277	2853.360148	22.997645
101.061710	2862.816151	23.002663
101.040931	2852.505469	23.007680
100.708974	2859.625648	23.012698
100.914120	2847.462851	23.017715
101.288819	2852.015048	23.022733
101.041704	2855.824854	23.027751
101.256675	2853.985269	23.032768
101.409128	2873.800294	23.037786
101.687166	2877.075090	23.042803
101.715876	2884.474177	23.047821
101.677862	2879.856560	23.052839
101.831162	2874.137890	23.057856
101.837215	2885.394192	23.062874
101.987407	2882.471932	23.067891
102.180986	2888.954676	23.072909
102.125182	2908.738078	23.077927
102.501219	2907.278153	23.082944
102.557332	2904.429738	23.087962
102.695630	2907.561915	23.092979
102.566698	2906.363563	23.097997
102.643366	2908.426721	23.103015
102.729376	2910.853323	23.108032
102.690385	2930.689485	23.113050
102.803328	2932.991936	23.118067
103.056812	2934.385217	23.123085
102.855448	2937.155884	23.128103
103.027544	2945.239195	23.133120
103.286476	2953.375461	23.138138
103.653787	2949.507321	23.143155
103.884213	2954.408660	23.148173
103.476692	2952.205551	23.153191
103.923436	2968.541361	23.158208
103.935385	2989.850396	23.163226
104.357192	2983.504110	23.168243
104.425729	2983.529074	23.173261
104.461104	2979.236314	23.178279
104.925708	2984.150470	23.183296
104.840811	2982.759765	23.188314
104.464192	2976.489762	23.193331
104.790341	2974.045091	23.198349
104.506046	2983.444249	23.203367
105.188484	2993.989378	23.208384
104.872050	3003.263543	23.213402
104.964377	3008.087361	23.218419
105.110295	3003.986153	23.223437
105.144795	3020.642263	23.228455
105.428771	3025.459948	23.233472
105.669342	3033.820183	23.238490
105.790049	3036.008755	23.243507
105.488580	3034.573187	23.248525
105.940612	3038.438164	23.253543
106.432736	3043.782469	23.258560
106.613744	3049.855118	23.263578
106.687922	3041.813052	23.268595
106.729287	3045.356618	23.273613
106.554401	3049.325000	23.278631
106.793728	3050.479275	23.283648
106.894371	3049.724049	23.288666
106.741585	3046.211705	23.293683
106.844993	3045.415860	23.298701
107.061607	3040.459160	23.303719
107.320730	3040.178529	23.308736
107.224678	3047.391244	23.313754
107.225437	3047.204969	23.318771
107.389561	3060.193655	23.323789
107.320463	3074.749849	23.328807
107.349364	3075.799581	23.333824
107.350182	3074.247419	23.338842
107.563235	3090.323202	23.343859
107.991747	3096.646653	23.348877
107.509817	3107.292895	23.353895
107.802816	3093.658530	23.358912
107.854438	3111.337196	23.363930
107.766652	3128.840912	23.368947
108.389163	3119.478374	23.373965
108.428415	3129.893054	23.378983
108.917559	3132.423829	23.384000
109.084711	3147.051223	23.389018
108.978109	3156.365547	23.394035
109.661844	3147.902002	23.399053
109.420439	3157.081150	23.404071
109.658971	3140.140473	23.409088
109.510844	3139.139001	23.414106
109.371935	3147.784981	23.419123
109.507360	3142.515675	23.424141
109.629984	3144.835061	23.429159
109.739159	3149.982936	23.434176
109.752675	3143.550232	23.439194
109.645881	3146.773041	23.444211
109.796854	3156.398299	23.449229
110.028722	3169.019919	23.454247
110.226232	3177.699203	23.459264
110.397460	3173.707552	23.464282
110.408219	3166.027138	23.469299
110.448253	3183.234922	23.474317
110.822782	3196.375126	23.479335
110.726641	3200.847884	23.484352
110.908113	3195.215782	23.489370
110.893938	3204.093923	23.494387
111.220124	3194.113406	23.499405
111.428454	3219.267799	23.504423
111.481252	3224.158077	23.509440
111.907665	3217.402231	23.514458
112.036944	3224.161536	23.519475
112.174927	3218.051143	23.524493
112.283552	3218.768755	23.529511
112.017441	3217.031615	23.534528
112.153407	3216.212260	23.539546
112.151674	3215.014873	23.544563
112.143828	3208.560086	23.549581
112.173591	3225.216016	23.554599
112.556590	3234.782434	23.559616
112.465466	3242.661421	23.564634
112.366267	3240.276894	23.569651
113.154581	3246.813306	23.574669
113.406540	3250.700832	23.579687
113.236053	3266.980076	23.584704
113.482299	3261.653795	23.589722
113.389674	3270.689073	23.594739
113.860758	3268.217211	23.599757
113.668099	3265.756412	23.604775
113.651209	3262.793234	23.609792
113.428333	3272.290675	23.614810
113.695304	3273.376604	23.619827
114.129586	3277.523745	23.624845
113.795774	3288.213704	23.629863
114.232809	3288.189866	23.634880
114.526082	3294.740141	23.639898
114.189937	3293.644970	23.644915
114.588519	3307.848724	23.649933
114.592886	3326.288295	23.654951
114.706993	3325.402860	23.659968
114.771930	3329.293807	23.664986
114.460632	3330.918836	23.670003
115.103661	3341.403004	23.675021
115.178809	3344.821346	23.680039
115.161968	3351.196191	23.685056
115.449479	3349.885939	23.690074
115.470703	3359.378850	23.695091
115.845413	3371.303287	23.700109
115.612853	3374.727300	23.705127
115.817296	3372.910661	23.710144
116.533796	3373.082708	23.715162
116.261356	3375.979011	23.720179
116.485567	3368.145429	23.725197
116.586401	3370.620442	23.730215
116.409335	3375.163741	23.735232
116.803970	3380.356962	23.740250
116.772733	3397.694118	23.745267
116.789799	3403.276273	23.750285
116.928308	3398.607620	23.755303
116.898134	3393.433765	23.760320
117.452021	3393.161814	23.765338
116.954628	3391.615719	23.770355
117.493397	3401.485228	23.775373
117.229985	3427.398846	23.780391
117.395249	3428.943803	23.785408
117.843851	3426.726063	23.790426
117.722143	3430.998764	23.795443
118.098143	3440.657029	23.800461
117.740532	3450.536770	23.805479
118.161882	3443.020553	23.810496
118.565072	3450.734331	23.815514
117.980448	3458.653001	23.820531
118.585026	3469.177877	23.825549
118.614619	3466.310127	23.830567
118.866657	3475.834588	23.835584
119.185899	3470.335109	23.840602
119.285557	3475.231488	23.845619
119.118034	3466.109008	23.850637
119.063339	3482.131874	23.855655
119.597636	3485.543923	23.860672
120.173990	3483.156976	23.865690
119.893629	3484.642236	23.870707
120.061571	3487.558967	23.875725
120.363616	3483.227038	23.880743
119.929511	3486.298175	23.885760
120.779311	3476.636350	23.890778
120.456471	3483.127272	23.895795
120.547555	3478.997220	23.900813
120.459240	3490.592060	23.905831
120.718916	3509.608944	23.910848
120.931872	3509.104820	23.915866
120.881118	3519.793747	23.920883
121.135396	3505.346438	23.925901
120.978744	3511.661415	23.930919
121.081654	3514.345582	23.935936
121.487774	3524.492280	23.940954
121.550702	3530.791779	23.945971
121.709223	3525.486627	23.950989
121.962632	3524.643875	23.956007
121.877624	3531.226954	23.961024
122.339843	3521.479644	23.966042
122.375207	3526.302028	23.971059
122.422887	3541.665014	23.976077
122.636277	3552.153913	23.981095
122.719356	3555.687539	23.986112
122.757502	3554.859949	23.991130
122.620784	3551.392474	23.996147
123.035865	3550.202441	24.001165
123.347405	3556.383616	24.006183
123.010140	3557.438091	24.011200
123.432828	3546.160112	24.016218
123.340262	3577.116401	24.021235
123.377703	3571.933261	24.026253
123.413442	3579.538626	24.031271
123.501676	3580.048975	24.036288
123.623626	3586.118225	24.041306
123.722114	3605.236724	24.046323
123.832126	3604.822879	24.051341
123.875855	3611.172446	24.056359
123.623367	3619.563833	24.061376
124.122773	3632.781775	24.066394
124.632737	3647.078437	24.071411
124.442124	3649.954942	24.076429
124.765836	3642.325252	24.081447
124.634570	3644.478058	24.086464
125.109095	3654.869455	24.091482
125.365934	3663.038728	24.096499
125.429245	3659.187672	24.101517
125.595658	3658.046677	24.106535
125.376964	3659.907620	24.111552
125.847925	3650.491111	24.116570
125.762156	3654.553566	24.121587
125.952727	3665.318403	24.126605
126.307603	3677.810607	24.131623
126.085184	3680.049779	24.136640
126.512871	3682.428990	24.141658
126.401580	3676.812898	24.146675
126.123663	3680.964266	24.151693
126.538118	3687.117823	24.156711
126.555650	3708.907293	24.161728
126.853374	3709.225068	24.166746
126.968137	3714.859673	24.171763
127.472789	3706.102603	24.176781
127.423297	3717.747884	24.181799
127.301217	3723.691819	24.186816
127.643622	3728.116928	24.191834
127.794736	3731.970083	24.196851
127.795848	3736.991930	24.201869
128.015548	3725.805311	24.206887
128.121907	3740.023977	24.211904
128.184334	3746.927666	24.216922
128.358634	3755.381162	24.221939
128.216495	3755.174830	24.226957
128.815237	3758.004539	24.231975
128.797555	3766.930044	24.236992
129.117933	3747.609875	24.242010
128.904332	3776.534346	24.247027
128.862093	3773.838690	24.252045
128.993392	3773.886735	24.257063
129.151103	3781.308597	24.262080
129.658058	3795.880341	24.267098
129.629458	3802.039570	24.272115
129.690551	3809.210868	24.277133
129.829805	3806.302062	24.282151
129.846666	3805.972934	24.287168
130.044898	3806.093768	24.292186
130.193068	3815.845506	24.297203
130.499033	3814.696358	24.302221
130.884490	3813.102493	24.307239
130.549333	3819.875947	24.312256
130.700701	3816.805662	24.317274
131.206589	3837.787192	24.322291
130.900468	3846.840428	24.327309
131.042435	3850.194268	24.332327
130.813268	3856.903333	24.337344
131.104818	3863.235992	24.342362
131.016954	3874.777491	24.347379
131.202592	3883.292574	24.352397
131.786881	3894.951186	24.357415
131.922442	3904.182943	24.362432
132.128773	3915.174904	24.367450
132.269811	3905.895160	24.372467
132.151371	3905.360445	24.377485
132.517336	3920.061963	24.382503
132.692092	3926.076533	24.387520
132.883898	3932.269412	24.392538
132.981542	3939.113410	24.397555
133.170523	3930.756562	24.402573
133.468950	3928.112370	24.407591
133.296481	3933.643403	24.412608
133.342838	3925.643291	24.417626
133.624220	3954.250674	24.422643
133.445204	3949.115058	24.427661
134.189393	3951.010352	24.432679
133.960562	3957.362658	24.437696
133.919783	3948.465012	24.442714
134.335438	3956.500650	24.447731
134.261259	3958.792889	24.452749
134.637474	3974.885884	24.457767
134.373788	3981.389662	24.462784
134.457015	3988.376247	24.467802
134.321728	3985.758961	24.472819
134.646392	4008.151247	24.477837
134.950143	4009.572926	24.482855
135.029549	4020.595425	24.487872
134.879177	4013.385435	24.492890
135.535198	4027.283799	24.497907
135.553251	4040.149035	24.502925
135.549018	4029.334760	24.507943
135.743962	4055.193218	24.512960
136.033062	4066.207808	24.517978
136.151561	4072.094718	24.522995
136.416621	4072.302144	24.528013
136.489000	4071.153850	24.533031
136.938345	4092.621536	24.538048
137.012197	4083.815089	24.543066
137.199900	4089.210945	24.548083
137.134587	4091.154436	24.553101
137.398322	4081.562891	24.558119
137.562249	4085.801082	24.563136
137.909949	4075.853853	24.568154
138.071048	4069.538090	24.573171
138.192422	4072.028715	24.578189
138.312346	4075.119675	24.583207
137.884564	4076.520716	24.588224
138.472530	4089.665716	24.593242
138.754068	4096.508477	24.598259
138.359142	4112.911989	24.603277
138.767338	4096.200108	24.608295
138.198282	4104.679995	24.613312
138.618286	4115.876918	24.618330
138.914239	4123.537908	24.623347
139.074438	4135.981201	24.628365
139.008687	4129.491125	24.633383
139.080752	4139.192662	24.638400
139.097748	4151.106830	24.643418
139.572269	4158.056274	24.648435
139.521733	4161.067580	24.653453
139.801841	4178.854924	24.658471
139.812360	4191.487635	24.663488
140.010032	4187.208627	24.668506
140.320105	4196.619574	24.673523
140.291163	4212.868882	24.678541
140.623385	4221.594173	24.683559
140.420213	4221.290833	24.688576
141.079795	4225.040636	24.693594
141.479072	4242.279100	24.698611
141.130932	4242.680190	24.703629
141.698082	4236.157742	24.708647
141.508719	4240.622209	24.713664
141.621445	4240.101187	24.718682
142.093174	4233.260624	24.723699
142.014120	4252.350241	24.728717
142.298263	4257.489992	24.733735
142.475322	4265.297529	24.738752
142.533022	4268.200370	24.743770
142.673039	4256.652487	24.748787
142.543833	4272.418372	24.753805
142.946864	4249.664423	24.758823
142.784761	4258.463698	24.763840
143.113294	4259.220557	24.768858
143.167148	4273.218046	24.773875
143.438316	4290.359642	24.778893
143.152665	4284.004350	24.783911
143.437420	4291.727917	24.788928
143.348088	4290.963133	24.793946
143.354349	4305.259919	24.798963
143.427235	4319.306275	24.803981
144.015091	4330.892172	24.808999
144.254161	4338.899752	24.814016
144.479209	4349.163596	24.819034
144.670788	4335.613857	24.824051
144.809631	4349.624120	24.829069
144.812797	4348.981051	24.834087
145.216411	4365.726722	24.839104
145.200579	4372.484953	24.844122
145.162578	4367.671584	24.849139
145.419454	4371.523533	24.854157
145.868408	4369.204016	24.859175
145.740072	4382.053604	24.864192
145.762372	4390.879127	24.869210
145.997078	4396.886316	24.874227
146.201491	4404.587014	24.879245
146.186298	4402.875925	24.884263
146.486310	4425.952539	24.889280
146.605709	4422.188879	24.894298
146.783015	4428.671809	24.899315
146.715622	4433.760348	24.904333
146.830461	4443.130524	24.909351
146.996174	4453.774405	24.914368
147.144993	4454.905971	24.919386
147.573284	4472.570673	24.924403
147.422760	4476.746048	24.929421
147.930137	4487.890971	24.934439
147.725798	4485.033018	24.939456
148.110546	4500.532120	24.944474
148.593936	4502.062714	24.949491
148.322866	4511.103833	24.954509
148.535635	4504.871485	24.959527
148.833636	4510.413825	24.964544
149.178240	4517.320360	24.969562
149.288801	4528.067141	24.974579
149.390927	4536.275480	24.979597
149.212265	4531.216006	24.984615
149.378588	4528.011587	24.989632
149.547209	4539.998604	24.994650
149.890369	4551.648014	24.999667
149.733906	4554.605265	25.004685
149.831799	4552.310765	25.009703
150.161157	4566.362136	25.014720
150.262225	4579.843324	25.019738
150.217943	4585.820381	25.024755
150.314531	4593.324021	25.029773
150.834668	4600.947345	25.034791
150.653710	4606.705258	25.039808
151.019028	4616.704277	25.044826
151.538838	4608.228509	25.049843
151.623420	4629.455688	25.054861
151.599088	4637.920494	25.059879
152.056432	4646.214206	25.064896
151.775797	4647.556281	25.069914
151.969767	4633.108078	25.074931
152.253748	4639.315905	25.079949
152.072274	4644.417098	25.084967
152.189496	4649.384574	25.089984
152.514198	4655.336011	25.095002
152.611504	4660.795072	25.100019
152.483776	4675.269525	25.105037
152.683422	4676.479324	25.110055
152.793688	4689.592870	25.115072
152.979586	4700.781717	25.120090
153.502779	4709.214196	25.125107
153.385717	4711.356132	25.130125
153.607935	4720.340907	25.135143
153.850656	4739.276248	25.140160
154.154075	4746.359028	25.145178
154.119179	4744.497590	25.150195
154.545718	4757.983328	25.155213
154.467805	4754.908292	25.160231
154.788752	4754.427601	25.165248
155.126463	4770.201741	25.170266
155.219765	4773.591007	25.175283
155.554060	4772.039386	25.180301
155.384182	4771.375332	25.185319
155.331779	4768.109418	25.190336
155.318146	4784.782853	25.195354
155.817152	4792.049066	25.200371
155.811043	4805.300108	25.205389
156.063003	4808.805665	25.210407
156.258998	4808.053473	25.215424
156.170045	4831.280922	25.220442
156.409991	4831.765016	25.225459
156.486296	4856.119711	25.230477
156.833098	4852.858572	25.235495
157.318869	4855.766260	25.240512
156.931185	4865.920814	25.245530
157.438073	4877.531549	25.250547
157.562325	4879.832024	25.255565
157.606827	4887.579122	25.260583
158.156416	4877.426278	25.265600
157.956501	4893.541568	25.270618
158.336992	4899.247592	25.275635
158.400956	4903.202492	25.280653
158.528230	4916.246468	25.285671
158.483245	4910.678023	25.290688
158.743519	4927.127485	25.295706
158.713572	4929.896108	25.300723
158.810082	4939.757907	25.305741
159.034636	4952.557414	25.310759
159.530404	4958.681477	25.315776
159.720315	4968.910591	25.320794
159.962521	4967.572665	25.325811
160.003884	4973.693205	25.330829
160.189894	4985.524106	25.335847
160.397351	4989.277281	25.340864
160.260351	4996.564611	25.345882
160.119712	5007.290300	25.350899
160.584967	5020.072853	25.355917
160.472880	5032.384730	25.360935
160.877839	5031.989358	25.365952
160.879742	5062.148507	25.370970
161.803581	5058.561038	25.375987
161.771075	5057.704900	25.381005
161.545416	5061.109229	25.386023
161.990987	5063.821993	25.391040
161.826961	5079.976423	25.396058
162.576693	5069.196491	25.401075
162.631682	5082.124197	25.406093
162.561238	5081.453119	25.411111
162.677179	5084.221245	25.416128
163.077063	5103.653958	25.421146
163.525056	5096.477510	25.426163
163.480544	5099.606922	25.431181
163.187171	5096.598991	25.436199
163.582004	5089.212401	25.441216
163.327438	5092.202531	25.446234
163.759354	5101.567075	25.451251
163.963102	5113.820429	25.456269
163.879109	5117.556515	25.461287
164.233906	5120.239425	25.466304
163.977604	5127.774964	25.471322
164.376959	5143.543999	25.476339
164.663641	5153.192518	25.481357
164.706161	5161.073180	25.486375
165.188323	5165.973316	25.491392
165.272087	5181.269319	25.496410
165.496509	5177.522747	25.501427
165.680913	5171.846140	25.506445
165.379794	5183.441228	25.511463
165.848807	5179.698268	25.516480
166.048232	5203.133699	25.521498
166.060573	5206.785339	25.526515
166.142637	5218.274487	25.531533
166.215466	5235.295584	25.536551
166.775626	5236.778106	25.541568
166.664063	5240.629046	25.546586
167.099718	5254.716206	25.551603
167.154369	5257.784340	25.556621
167.145626	5266.568238	25.561639
167.650118	5279.142885	25.566656
167.832154	5282.324613	25.571674
167.770601	5296.587058	25.576691
167.794695	5294.881181	25.581709
167.853517	5309.505689	25.586727
168.284186	5310.403213	25.591744
168.534607	5327.600570	25.596762
168.635490	5341.220269	25.601779
168.955110	5352.687515	25.606797
169.098275	5349.646646	25.611815
169.615802	5354.770964	25.616832
169.521489	5367.755912	25.621850
169.637655	5366.041874	25.626867
170.067329	5367.016749	25.631885
170.584401	5359.108103	25.636903
170.697087	5351.016740	25.641920
170.743202	5357.762776	25.646938
170.865893	5354.623696	25.651955
171.137318	5367.774136	25.656973
171.199462	5379.441544	25.661991
171.456264	5379.157328	25.667008
171.503308	5376.356043	25.672026
171.611231	5375.003297	25.677044
171.945748	5369.972008	25.682061
171.694750	5379.029988	25.687079
171.935409	5373.996909	25.692096
171.870036	5397.399283	25.697114
172.113845	5405.150658	25.702132
172.204135	5396.838515	25.707149
172.074332	5417.306779	25.712167
172.348668	5429.243894	25.717184
172.366679	5445.852145	25.722202
172.697145	5453.185949	25.727220
173.100452	5461.881264	25.732237
172.735775	5481.174809	25.737255
173.242715	5491.184021	25.742272
173.587316	5495.618725	25.747290
173.725502	5513.375158	25.752308
173.927956	5521.543775	25.757325
174.050719	5519.415139	25.762343
174.281549	5527.364047	25.767360
174.428251	5541.637130	25.772378
174.529317	5546.208252	25.777396
174.913077	5539.835352	25.782413
174.773851	5556.224017	25.787431
175.057681	5568.626714	25.792448
175.253577	5576.517635	25.797466
175.646100	5576.982009	25.802484
176.057548	5586.122615	25.807501
175.637674	5599.975242	25.812519
176.140711	5594.363088	25.817536
176.294163	5598.890111	25.822554
176.332214	5602.853414	25.827572
176.555018	5613.071989	25.832589
176.930166	5622.310775	25.837607
176.925981	5623.070017	25.842624
176.929955	5638.762449	25.847642
176.986450	5648.139064	25.852660
177.288728	5651.269457	25.857677
177.453825	5678.376003	25.862695
178.052182	5681.418795	25.867712
178.079069	5685.058686	25.872730
177.776622	5695.122472	25.877748
178.695836	5703.152049	25.882765
178.557230	5714.128339	25.887783
178.737482	5710.773307	25.892800
178.733859	5728.877165	25.897818
178.789094	5744.314694	25.902836
179.268577	5753.176348	25.907853
179.586689	5765.842099	25.912871
179.964346	5770.809347	25.917888
180.066489	5765.294217	25.922906
180.175421	5771.678757	25.927924
180.596800	5772.972441	25.932941
180.577634	5793.238575	25.937959
180.642506	5801.097741	25.942976
181.137528	5792.170211	25.947994
180.856078	5794.033912	25.953012
181.082807	5804.859998	25.958029
181.438796	5819.678368	25.963047
181.311232	5822.700379	25.968064
181.646115	5829.434255	25.973082
181.753517	5844.841981	25.978100
182.210276	5842.816321	25.983117
182.069772	5850.436997	25.988135
182.070883	5858.975432	25.993152
182.565602	5873.019501	25.998170
182.234462	5882.490356	26.003188
183.311897	5898.556670	26.008205
183.156126	5903.610692	26.013223
183.182468	5900.576456	26.018240
183.358415	5927.375250	26.023258
183.131187	5932.155993	26.028276
183.674379	5939.641475	26.033293
183.828492	5964.567051	26.038311
184.188014	5966.698781	26.043328
184.036629	5972.607455	26.048346
184.489855	5996.694368	26.053364
184.858964	5993.241853	26.058381
185.121620	5995.452633	26.063399
185.374216	6016.258478	26.068416
185.762327	6020.729448	26.073434
186.159229	6023.057417	26.078452
186.142039	6017.663558	26.083469
185.935915	6014.565393	26.088487
185.952405	6023.426659	26.093504
186.398379	6039.993041	26.098522
186.443013	6047.074357	26.103540
186.855318	6043.305144	26.108557
186.895961	6045.259687	26.113575
187.300110	6047.465954	26.118592
187.704457	6062.779840	26.123610
187.413940	6069.587421	26.128628
187.643552	6065.203381	26.133645
187.457709	6061.862411	26.138663
187.423918	6068.053314	26.143680
187.835963	6082.080540	26.148698
187.725989	6092.441942	26.153716
188.341655	6117.201561	26.158733
188.284829	6127.485664	26.163751
188.719509	6142.179468	26.168768
188.874239	6147.022277	26.173786
189.022369	6156.119380	26.178804
189.281518	6158.544211	26.183821
189.208392	6180.915657	26.188839
189.540735	6188.968602	26.193856
189.844973	6198.900768	26.198874
189.830928	6215.079573	26.203892
190.550139	6220.401567	26.208909
190.486077	6234.306110	26.213927
190.623289	6243.824880	26.218944
190.742994	6246.826516	26.223962
190.979027	6255.868168	26.228980
191.258018	6267.663375	26.233997
191.185437	6281.864734	26.239015
191.254156	6291.883205	26.244032
191.889366	6303.012988	26.249050
191.883433	6309.134787	26.254068
192.389562	6321.100369	26.259085
192.553837	6332.397136	26.264103
192.162122	6338.959301	26.269120
193.163000	6346.450339	26.274138
193.092630	6364.164277	26.279156
193.368400	6359.136102	26.284173
193.535169	6369.210067	26.289191
193.800839	6383.476030	26.294208
194.145854	6378.409607	26.299226
194.170903	6392.341283	26.304244
194.544282	6383.727351	26.309261
194.626287	6401.234161	26.314279
194.671096	6412.523195	26.319296
195.024323	6411.458202	26.324314
194.795475	6412.924169	26.329332
195.119315	6424.779019	26.334349
195.126336	6434.579378	26.339367
195.559370	6443.652325	26.344384
195.727393	6458.374814	26.349402
195.733717	6470.987203	26.354420
196.088993	6480.549568	26.359437
196.406925	6497.368408	26.364455
196.293014	6502.512571	26.369472
196.738452	6514.985352	26.374490
196.966234	6532.390197	26.379508
197.153343	6533.999982	26.384525
197.609373	6549.265615	26.389543
197.678278	6560.282965	26.394560
197.987739	6564.880534	26.399578
197.936875	6570.117463	26.404596
198.471077	6565.596223	26.409613
198.577870	6591.842845	26.414631
198.772705	6586.857929	26.419648
199.156124	6581.086438	26.424666
198.957901	6593.768230	26.429684
199.405882	6598.728039	26.434701
199.772317	6615.659487	26.439719
199.631469	6613.085213	26.444736
199.670418	6616.493326	26.449754
199.591111	6614.062457	26.454772
200.333924	6632.536852	26.459789
200.502334	6636.303187	26.464807
200.418656	6646.719672	26.469824
200.639374	6644.345464	26.474842
200.774455	6660.139290	26.479860
200.826854	6667.755204	26.484877
200.875989	6682.869356	26.489895
200.770439	6698.807814	26.494912
201.346015	6711.590024	26.499930
201.512392	6733.124703	26.504948
201.450582	6739.620603	26.509965
202.348433	6752.440865	26.514983
202.273304	6770.177310	26.520000
202.433442	6766.046392	26.525018
202.355534	6800.923610	26.530036
202.815568	6795.457575	26.535053
203.162677	6811.829253	26.540071
203.037124	6826.305310	26.545088
203.836217	6832.804451	26.550106
203.781747	6840.789437	26.555124
203.908195	6845.563102	26.560141
204.589266	6854.647999	26.565159
204.715405	6867.073884	26.570176
205.099859	6864.384254	26.575194
204.663852	6871.762112	26.580212
205.338830	6882.580898	26.585229
205.449420	6893.183568	26.590247
205.762608	6900.934435	26.595264
206.042805	6898.968595	26.600282
206.097031	6916.427798	26.605300
206.487962	6916.541972	26.610317
206.792881	6919.583966	26.615335
206.695833	6920.399602	26.620352
207.191629	6940.107778	26.625370
207.318486	6954.642989	26.630388
207.112619	6948.560905	26.635405
207.061730	6951.757114	26.640423
207.299267	6973.242531	26.645440
207.413654	6984.639393	26.650458
207.729653	7003.144706	26.655476
207.953457	7019.415710	26.660493
208.481669	7038.547580	26.665511
208.618142	7040.428095	26.670528
209.000490	7055.311791	26.675546
209.267057	7067.139583	26.680564
209.271674	7068.611071	26.685581
209.481838	7075.379519	26.690599
209.454996	7101.048897	26.695616
209.897961	7104.869930	26.700634
210.527591	7118.656476	26.705652
210.422050	7126.591771	26.710669
210.651935	7127.429701	26.715687
210.617533	7139.648435	26.720704
211.057767	7148.730049	26.725722
210.987078	7153.347398	26.730740
211.189349	7169.206226	26.735757
211.574751	7176.597120	26.740775
211.373303	7192.707907	26.745792
212.396759	7205.758231	26.750810
212.721093	7210.689868	26.755828
212.772681	7215.868303	26.760845
213.015886	7218.879612	26.765863
213.274381	7238.637683	26.770880
213.200077	7233.245776	26.775898
213.602172	7248.398135	26.780916
213.349300	7251.261567	26.785933
213.983357	7266.023449	26.790951
213.962163	7277.387040	26.795968
214.001935	7272.051853	26.800986
214.254619	7286.727227	26.806004
214.260349	7297.368005	26.811021
214.581159	7308.922336	26.816039
214.613021	7316.049656	26.821056
214.760790	7327.486136	26.826074
215.008203	7343.124201	26.831092
215.156851	7362.329536	26.836109
215.555940	7362.087116	26.841127
215.375290	7388.507093	26.846144
215.647754	7389.500254	26.851162
216.030170	7414.203633	26.856180
216.566779	7423.684566	26.861197
217.010139	7439.070523	26.866215
216.988763	7451.187302	26.871232
217.571675	7454.856861	26.876250
217.715950	7473.666056	26.881268
218.169443	7472.266958	26.886285
218.792217	7469.985977	26.891303
218.580828	7480.072835	26.896320
218.493827	7481.142837	26.901338
218.717815	7495.403312	26.906356
218.897744	7498.348743	26.911373
219.418082	7503.280322	26.916391
219.449707	7524.338981	26.921408
219.362775	7532.009094	26.926426
219.818138	7540.874964	26.931444
219.666693	7563.111656	26.936461
220.039732	7562.442675	26.941479
220.386888	7579.279095	26.946496
220.377770	7590.384906	26.951514
220.851485	7599.068176	26.956532
220.927817	7614.336251	26.961549
221.495556	7615.790192	26.966567
221.218872	7649.286672	26.971584
221.982212	7654.211157	26.976602
222.117670	7652.856814	26.981620
222.135869	7677.814670	26.986637
222.747558	7686.286098	26.991655
222.483026	7697.376762	26.996672
222.481852	7709.698348	27.001690
222.863962	7721.478357	27.006708
223.459914	7735.755458	27.011725
223.915494	7738.721472	27.016743
223.878896	7744.843385	27.021760
223.761671	7758.335061	27.026778
224.191085	7764.865069	27.031796
224.526794	7781.495642	27.036813
224.900033	7792.034954	27.041831
224.701771	7800.261631	27.046848
225.195385	7807.074057	27.051866
225.615101	7816.807740	27.056884
225.858018	7820.284751	27.061901
225.953416	7825.987839	27.066919
226.013307	7846.851618	27.071936
226.263554	7841.778368	27.076954
226.581282	7851.013003	27.081972
226.622230	7877.905969	27.086989
227.052845	7880.393274	27.092007
226.995915	7894.168901	27.097024
227.291318	7903.544324	27.102042
227.508817	7912.166988	27.107060
227.755352	7932.679383	27.112077
227.896790	7939.037361	27.117095
228.282085	7945.212396	27.122112
228.248509	7967.191460	27.127130
228.809403	7974.263798	27.132148
228.520037	7998.538914	27.137165
229.141725	8004.348725	27.142183
229.003620	8003.168824	27.147200
229.129133	8021.044382	27.152218
229.410520	8037.929198	27.157236
229.602054	8066.579385	27.162253
230.119674	8068.015672	27.167271
230.016427	8094.968321	27.172288
230.168743	8097.300858	27.177306
230.905484	8120.714680	27.182324
231.262656	8124.805390	27.187341
231.576753	8133.170351	27.192359
231.739638	8148.389951	27.197376
231.773415	8150.386853	27.202394
232.006217	8159.304879	27.207412
232.389156	8179.442897	27.212429
232.339787	8172.660140	27.217447
232.722306	8198.544740	27.222464
233.018451	8205.692516	27.227482
233.363055	8225.479308	27.232500
233.384190	8244.396447	27.237517
234.075410	8246.271141	27.242535
233.806467	8264.497428	27.247552
234.405290	8271.291065	27.252570
234.571137	8274.683255	27.257588
234.698493	8295.999642	27.262605
235.201557	8290.614208	27.267623
234.948214	8312.504875	27.272640
235.351142	8317.375798	27.277658
235.864328	8334.818875	27.282676
236.087055	8356.135309	27.287693
236.047093	8360.326480	27.292711
236.594160	8371.942601	27.297728
236.554069	8380.320633	27.302746
237.054030	8385.392931	27.307764
237.028422	8407.432725	27.312781
237.411548	8407.507248	27.317799
237.408855	8408.558628	27.322816
237.683478	8438.428543	27.327834
238.354293	8439.793031	27.332852
238.196533	8469.020882	27.337869
238.531042	8476.017485	27.342887
238.913402	8486.358025	27.347904
238.681342	8499.623558	27.352922
239.154540	8504.540412	27.357940
239.389820	8525.686417	27.362957
239.601278	8534.705868	27.367975
239.581972	8548.953206	27.372992
239.984393	8567.702842	27.378010
240.233915	8587.390023	27.383028
240.218194	8602.752270	27.388045
240.749967	8616.645338	27.393063
241.238328	8626.379972	27.398080
241.531941	8649.204637	27.403098
241.915229	8643.459217	27.408116
242.058994	8651.100343	27.413133
242.322232	8669.651780	27.418151
242.736551	8680.283351	27.423168
242.372257	8684.562167	27.428186
243.017306	8692.100641	27.433204
243.180761	8705.836547	27.438221
243.293986	8720.789986	27.443239
243.695282	8728.963583	27.448256
243.858303	8739.205888	27.453274
244.354562	8749.123625	27.458292
244.149491	8762.203723	27.463309
245.158217	8752.690871	27.468327
245.592594	8761.045706	27.473344
245.328765	8764.150696	27.478362
245.926932	8772.480788	27.483380
246.236421	8773.978381	27.488397
246.532435	8777.689444	27.493415
246.566231	8763.373508	27.498432
246.584524	8771.111874	27.503450
246.630572	8769.370481	27.508468
246.915024	8781.338388	27.513485
247.064526	8791.152060	27.518503
246.947397	8798.088071	27.523520
247.021586	8821.254167	27.528538
247.549530	8821.181044	27.533556
247.602081	8853.658962	27.538573
248.029687	8864.139570	27.543591
247.992263	8880.608544	27.548608
248.254473	8906.321206	27.553626
248.704076	8921.639032	27.558644
248.997380	8937.606656	27.563661
249.354238	8955.804976	27.568679
249.432153	8962.787549	27.573696
249.419464	8988.087364	27.578714
249.933716	8993.920843	27.583732
250.026012	9024.306512	27.588749
250.224536	9034.420238	27.593767
250.770115	9049.640371	27.598784
250.848586	9057.060107	27.603802
251.133887	9081.326027	27.608820
251.389299	9110.479565	27.613837
251.462522	9123.456383	27.618855
252.282311	9138.394091	27.623872
252.224345	9153.091095	27.628890
252.876157	9163.374081	27.633908
252.995860	9184.972581	27.638925
253.535347	9183.566989	27.643943
253.876296	9193.788011	27.648960
253.809237	9205.175531	27.653978
254.445286	9210.449300	27.658996
254.427444	9225.350854	27.664013
254.544478	9225.923193	27.669031
254.887798	9245.171045	27.674048
255.084722	9263.306382	27.679066
255.383763	9269.003062	27.684084
255.779832	9288.332829	27.689101
256.039957	9290.555527	27.694119
256.358702	9290.353175	27.699136
256.322982	9310.785653	27.704154
256.538991	9319.010706	27.709172
256.916655	9338.446781	27.714189
256.768290	9347.825612	27.719207
257.408759	9363.027187	27.724224
257.743486	9380.931083	27.729242
258.032980	9379.859913	27.734260
258.127460	9405.986370	27.739277
257.972894	9417.573656	27.744295
258.634341	9427.666149	27.749312
258.443541	9446.405510	27.754330
259.157603	9467.166270	27.759348
259.290399	9481.069414	27.764365
259.615496	9495.206227	27.769383
259.918578	9506.608320	27.774400
260.032923	9534.735849	27.779418
260.352331	9541.524292	27.784436
260.516935	9549.074953	27.789453
260.441681	9566.806641	27.794471
261.073614	9585.541541	27.799488
261.140916	9603.184285	27.804506
261.598685	9624.229528	27.809524
261.577511	9640.985715	27.814541
262.027058	9658.360419	27.819559
262.493999	9659.283725	27.824576
262.595541	9685.733255	27.829594
263.153556	9677.542354	27.834612
262.973834	9695.139430	27.839629
263.473964	9714.769974	27.844647
264.351244	9711.199471	27.849664
264.334916	9720.135187	27.854682
264.780616	9725.783332	27.859700
264.864828	9739.526941	27.864717
265.326801	9736.491559	27.869735
265.425513	9737.207967	27.874752
265.178508	9761.885242	27.879770
265.792844	9763.712194	27.884788
265.985483	9779.738288	27.889805
266.062238	9795.677225	27.894823
266.529335	9795.103676	27.899840
266.632617	9815.886422	27.904858
266.866029	9825.232272	27.909876
267.236866	9849.140136	27.914893
266.909173	9856.171329	27.919911
267.318972	9876.462242	27.924928
267.591484	9905.299268	27.929946
268.054746	9919.804342	27.934964
268.376476	9941.145891	27.939981
268.472087	9961.415650	27.944999
268.748032	9969.882431	27.950016
268.967237	9993.252318	27.955034
269.412857	10020.760997	27.960052
270.025002	10037.110244	27.965069
269.983651	10044.830734	27.970087
270.448036	10065.312169	27.975104
270.789424	10080.352009	27.980122
271.211512	10097.048693	27.985140
271.709321	10111.289816	27.990157
271.560655	10127.973074	27.995175
272.142125	10141.943545	28.000192
272.198276	10153.651682	28.005210
272.631176	10158.922369	28.010228
273.031698	10176.202545	28.015245
272.973493	10182.468410	28.020263
273.218923	10199.011665	28.025280
273.413836	10213.362891	28.030298
273.489090	10225.513829	28.035316
273.610381	10247.924960	28.040333
273.732519	10264.740009	28.045351
274.513484	10278.299419	28.050368
274.608068	10304.603793	28.055386
274.681062	10318.423808	28.060404
275.186610	10338.682912	28.065421
275.716298	10352.873279	28.070439
276.129463	10382.469413	28.075456
275.957541	10396.853948	28.080474
276.291631	10407.156454	28.085492
276.558834	10422.661115	28.090509
277.191400	10447.716973	28.095527
277.376076	10452.671164	28.100544
277.589247	10476.418553	28.105562
278.276946	10483.267764	28.110580
278.550607	10496.338569	28.115597
279.059971	10510.035310	28.120615
279.271784	10502.145533	28.125632
279.362340	10520.501584	28.130650
279.640967	10531.800520	28.135668
280.113486	10538.880759	28.140685
280.351581	10541.160854	28.145703
280.632271	10551.892215	28.150720
280.986312	10580.054377	28.155738
281.282713	10562.669615	28.160756
281.181345	10575.875041	28.165773
281.193223	10580.083420	28.170791
281.033990	10591.524205	28.175808
281.020317	10605.857520	28.180826
281.758878	10627.500487	28.185844
282.084019	10647.866264	28.190861
282.019763	10672.560376	28.195879
282.604493	10681.965177	28.200896
282.725663	10694.828179	28.205914
282.929823	10730.162819	28.210932
283.312534	10734.858204	28.215949
283.604878	10759.242885	28.220967
284.116308	10773.985783	28.225984
284.434444	10790.120532	28.231002
284.569319	10816.398587	28.236020
285.203065	10822.305143	28.241037
285.129586	10858.256428	28.246055
285.800078	10858.961759	28.251072
286.020639	10894.049806	28.256090
286.209343	10895.471479	28.261108
286.726203	10911.742059	28.266125
286.692786	10929.955220	28.271143
287.340841	10948.055604	28.276160
287.471443	10955.257227	28.281178
287.590537	10974.784567	28.286196
287.727757	10992.244717	28.291213
288.376260	11007.913735	28.296231
288.426858	11030.441653	28.301248
288.839297	11040.904141	28.306266
289.467884	11062.318506	28.311284
289.856161	11076.811040	28.316301
289.826805	11091.906890	28.321319
289.913571	11110.585691	28.326336
290.389818	11126.117883	28.331354
290.659840	11141.859132	28.336372
291.272309	11146.816002	28.341389
291.097808	11166.362230	28.346407
291.627757	11183.749704	28.351424
292.009977	11192.253904	28.356442
292.185737	11196.526711	28.361460
292.610949	11211.608888	28.366477
292.351713	11230.642916	28.371495
292.591965	11256.515033	28.376512
293.332869	11279.159099	28.381530
293.361888	11288.224480	28.386548
293.792261	11322.164663	28.391565
293.774722	11332.293539	28.396583
294.408768	11352.174164	28.401600
294.606275	11367.585694	28.406618
294.643495	11384.030688	28.411636
295.333821	11406.174330	28.416653
295.485361	11436.128495	28.421671
295.669305	11445.737177	28.426688
296.389073	11466.724134	28.431706
296.335744	11490.347728	28.436724
297.146859	11503.911856	28.441741
297.130897	11511.330233	28.446759
297.500549	11524.680656	28.451776
297.927940	11535.843793	28.456794
297.927460	11562.771053	28.461812
298.250912	11570.892809	28.466829
298.386021	11595.397750	28.471847
299.005764	11610.462284	28.476864
299.235042	11628.059159	28.481882
299.354409	11644.152024	28.486900
299.795600	11659.810294	28.491917
299.952405	11679.239270	28.496935
300.439520	11692.245774	28.501952
300.609811	11704.020448	28.506970
300.860397	11725.274497	28.511988
301.295507	11728.908864	28.517005
301.221975	11753.751133	28.522023
301.478884	11770.220038	28.527040
302.274051	11778.753899	28.532058
302.064091	11795.624722	28.537076
302.249552	11821.795185	28.542093
302.449811	11853.656674	28.547111
302.602486	11852.191193	28.552128
303.272883	11883.976502	28.557146
303.692080	11905.180817	28.562164
304.139078	11933.144007	28.567181
304.447989	11943.507607	28.572199
304.607948	11965.832777	28.577216
304.965662	11984.836484	28.582234
305.196908	12014.959747	28.587252
305.839772	12019.150732	28.592269
306.107838	12040.449576	28.597287
306.276041	12053.160897	28.602304
306.531058	12076.980139	28.607322
306.717346	12103.023276	28.612340
307.366956	12115.213728	28.617357
307.517153	12136.678762	28.622375
307.932017	12159.034495	28.627392
308.063705	12173.242707	28.632410
308.440502	12188.423634	28.637428
308.837053	12205.304803	28.642445
309.073302	12243.351054	28.647463
309.434533	12247.138019	28.652480
309.851321	12264.509144	28.657498
310.322548	12296.042998	28.662516
310.621083	12303.455382	28.667533
310.910650	12325.256894	28.672551
310.810647	12340.201708	28.677568
311.534492	12353.675417	28.682586
311.604936	12374.900251	28.687604
312.054329	12400.706486	28.692621
312.347631	12409.183498	28.697639
312.703522	12430.496684	28.702656
312.839577	12450.234162	28.707674
313.369343	12468.644220	28.712692
313.494101	12487.449116	28.717709
314.068483	12508.229839	28.722727
313.983591	12524.239193	28.727744
314.592764	12553.651638	28.732762
314.733359	12567.950123	28.737780
315.178243	12586.703725	28.742797
315.208020	12608.045906	28.747815
315.492966	12632.387357	28.752832
316.158173	12652.147811	28.757850
316.226401	12667.309344	28.762868
316.737120	12675.616560	28.767885
316.877965	12700.082821	28.772903
317.023068	12724.488529	28.777920
318.012884	12754.035324	28.782938
318.206014	12761.586710	28.787956
318.608031	12778.688199	28.792973
318.689050	12793.800456	28.797991
319.284688	12808.602195	28.803008
319.343376	12818.090591	28.808026
319.411505	12844.107195	28.813044
319.928785	12858.304190	28.818061
320.163471	12872.226484	28.823079
320.170281	12907.920021	28.828096
320.762918	12922.005317	28.833114
321.007908	12950.509566	28.838132
321.188407	12968.577715	28.843149
321.303716	12983.656106	28.848167
321.575597	13004.805871	28.853184
321.909598	13018.740219	28.858202
322.293296	13043.803477	28.863220
322.822581	13062.029905	28.868237
323.397836	13084.254779	28.873255
323.152318	13116.621180	28.878272
323.989869	13137.937522	28.883290
323.905864	13155.950374	28.888308
324.797104	13178.359469	28.893325
324.690878	13199.847859	28.898343
324.722227	13212.901080	28.903360
325.621368	13234.527273	28.908378
325.424018	13263.242390	28.913396
325.717218	13276.223955	28.918413
326.191805	13294.270582	28.923431
326.380762	13329.725291	28.928448
326.898493	13351.101151	28.933466
326.961255	13381.420306	28.938484
327.472828	13399.987301	28.943501
328.276072	13434.976519	28.948519
328.328632	13457.430252	28.953536
328.841520	13470.495386	28.958554
329.173383	13501.752057	28.963572
329.309179	13511.040553	28.968589
330.089828	13540.497322	28.973607
330.328330	13555.210712	28.978624
330.748654	13572.418749	28.983642
331.144945	13594.568351	28.988660
331.281108	13615.765011	28.993677
331.933329	13633.573007	28.998695
331.673349	13652.367278	29.003712
332.597425	13667.105987	29.008730
332.829848	13682.726694	29.013748
333.033088	13709.655304	29.018765
333.302826	13721.460685	29.023783
333.239775	13740.471471	29.028800
333.870697	13757.810329	29.033818
334.190571	13789.033287	29.038836
334.857516	13808.353580	29.043853
334.869252	13818.535893	29.048871
334.825833	13843.587545	29.053888
335.588779	13864.278906	29.058906
335.892022	13902.174523	29.063924
336.175252	13914.154324	29.068941
336.953259	13936.001657	29.073959
336.926734	13964.213770	29.078976
337.278813	13976.207438	29.083994
337.579369	14010.830350	29.089012
337.889246	14031.489740	29.094029
337.993078	14056.786848	29.099047
338.186338	14083.508113	29.104064
338.730892	14094.815958	29.109082
339.032282	14126.260111	29.114100
339.344550	14154.964941	29.119117
340.070095	14177.557293	29.124135
340.351463	14208.825250	29.129152
340.838850	14219.846347	29.134170
340.978186	14243.598069	29.139188
340.963027	14262.896255	29.144205
341.624667	14283.266065	29.149223
341.730054	14312.282796	29.154240
342.482654	14329.048929	29.159258
342.570136	14351.483924	29.164276
342.865049	14382.368564	29.169293
343.295817	14399.938241	29.174311
343.528927	14425.247618	29.179328
344.120850	14441.183079	29.184346
344.505585	14457.405018	29.189364
344.861138	14475.185809	29.194381
345.482697	14489.523004	29.199399
345.279290	14506.291513	29.204416
345.891472	14515.506463	29.209434
346.055136	14538.195462	29.214452
346.079723	14565.815425	29.219469
346.319152	14580.277412	29.224487
346.508852	14610.971854	29.229504
346.990021	14625.048707	29.234522
347.658568	14652.407780	29.239540
347.760544	14688.357383	29.244557
348.407158	14705.972046	29.249575
348.650343	14742.390137	29.254592
348.994423	14759.033617	29.259610
349.354898	14786.467544	29.264628
349.364061	14813.173184	29.269645
349.938262	14825.792678	29.274663
350.441805	14871.495361	29.279680
350.650141	14879.872669	29.284698
351.182161	14903.361764	29.289716
351.516668	14934.518287	29.294733
351.771731	14956.303808	29.299751
351.989222	14988.359273	29.304768
352.246537	15019.675313	29.309786
352.856757	15042.448713	29.314804
353.157539	15066.707636	29.319821
353.655764	15088.527165	29.324839
354.018864	15120.148995	29.329856
354.487239	15145.017054	29.334874
354.760644	15166.661118	29.339892
355.498981	15185.313978	29.344909
355.637683	15204.135452	29.349927
356.094729	15234.671754	29.354944
356.512132	15245.062060	29.359962
356.551544	15272.914026	29.364980
356.474949	15298.532919	29.369997
357.067313	15315.629208	29.375015
357.767366	15341.332410	29.380032
357.998211	15366.430832	29.385050
358.114153	15390.818547	29.390068
358.891173	15427.742440	29.395085
359.304995	15447.724425	29.400103
359.366461	15471.724082	29.405120
359.922807	15495.310874	29.410138
360.207599	15515.854922	29.415156
360.349049	15550.652422	29.420173
361.351946	15560.619759	29.425191
361.720340	15589.680330	29.430208
361.591572	15601.508889	29.435226
362.130229	15621.549233	29.440244
362.450789	15655.016960	29.445261
363.125170	15669.638044	29.450279
363.367908	15701.017688	29.455296
363.447731	15724.529209	29.460314
364.077167	15741.900369	29.465332
364.199589	15767.023651	29.470349
364.870387	15788.202409	29.475367
365.029134	15813.099081	29.480384
365.423938	15843.063620	29.485402
365.812751	15856.540524	29.490420
366.225634	15889.957196	29.495437
366.458885	15900.403615	29.500455
366.522106	15929.258370	29.505472
367.121145	15948.121147	29.510490
367.496668	15973.111433	29.515508
367.765397	16009.704637	29.520525
368.395825	16016.808438	29.525543
368.530047	16041.156260	29.530560
368.923649	16055.218889	29.535578
369.442083	16079.090209	29.540596
369.659842	16106.464841	29.545613
370.279095	16115.651157	29.550631
370.120469	16146.023085	29.555648
370.598113	16162.191928	29.560666
371.003270	16187.198126	29.565684
371.010235	16215.481060	29.570701
371.291798	16243.504227	29.575719
371.975624	16269.118569	29.580736
372.196628	16306.603025	29.585754
372.508319	16340.915328	29.590772
372.622843	16373.222236	29.595789
373.200195	16395.894193	29.600807
373.263074	16426.070774	29.605824
373.473980	16462.080299	29.610842
374.140101	16496.476129	29.615860
374.537152	16540.010058	29.620877
374.924681	16562.018524	29.625895
375.125854	16604.308259	29.630912
375.532272	16636.529542	29.635930
376.235882	16677.101710	29.640948
376.631855	16714.606997	29.645965
377.246319	16731.887106	29.650983
377.293892	16775.031825	29.656000
378.104280	16799.412300	29.661018
378.600843	16832.337837	29.666036
378.979164	16855.366505	29.671053
379.703846	16892.958086	29.676071
379.978809	16911.989097	29.681088
380.366575	16941.168640	29.686106
380.630465	16961.315989	29.691124
380.929906	16983.851896	29.696141
381.791075	17001.955277	29.701159
381.952312	17028.697653	29.706176
382.312636	17048.004735	29.711194
382.605376	17072.548524	29.716212
382.868256	17098.066730	29.721229
383.268600	17112.195350	29.726247
383.572918	17144.448707	29.731264
383.861847	17182.601724	29.736282
384.298796	17208.710790	29.741300
384.511668	17232.815627	29.746317
384.715661	17253.431957	29.751335
385.278954	17295.393972	29.756352
385.747794	17336.794782	29.761370
386.215394	17351.312868	29.766388
386.495145	17396.506283	29.771405
386.758202	17421.446436	29.776423
387.252308	17452.221890	29.781440
387.642718	17485.733781	29.786458
388.298523	17509.798819	29.791476
388.361311	17537.089541	29.796493
389.045884	17562.161921	29.801511
389.452470	17589.548739	29.806528
389.718943	17631.217077	29.811546
390.169224	17642.905543	29.816564
390.764478	17677.063337	29.821581
390.904523	17710.680172	29.826599
391.486681	17733.679480	29.831616
391.728016	17766.135210	29.836634
392.359044	17786.054128	29.841652
392.848670	17823.803376	29.846669
393.146803	17835.409964	29.851687
393.317226	17865.355396	29.856704
393.528985	17888.286953	29.861722
394.208985	17906.255790	29.866740
394.356928	17928.070839	29.871757
394.672784	17958.217794	29.876775
395.167316	17982.152569	29.881792
395.350329	18015.879563	29.886810
395.840635	18038.388468	29.891828
396.032220	18066.800064	29.896845
396.161913	18097.088429	29.901863
396.749889	18123.129800	29.906880
396.960203	18158.328093	29.911898
397.608682	18189.714663	29.916916
397.578401	18223.612949	29.921933
398.404543	18258.800971	29.926951
398.831057	18300.143399	29.931968
399.126545	18325.204078	29.936986
399.620238	18365.454113	29.942004
399.661773	18402.578890	29.947021
400.097091	18426.590314	29.952039
401.194421	18462.304561	29.957056
401.496837	18500.690107	29.962074
402.093597	18530.712788	29.967092
402.113035	18545.219384	29.972109
402.652558	18583.012542	29.977127
403.161694	18612.028323	29.982144
403.203668	18649.607598	29.987162
403.883723	18666.916710	29.992180
404.272737	18710.117137	29.997197
404.294622	18747.608521	30.002215
405.127330	18765.866737	30.007232
405.534740	18808.851550	30.012250
406.096763	18840.862179	30.017268
406.218331	18875.163884	30.022285
406.687859	18902.991747	30.027303
407.581234	18927.328518	30.032320
407.481601	18966.727568	30.037338
408.047679	18994.842293	30.042356
408.597386	19021.391154	30.047373
409.043564	19051.523248	30.052391
409.191003	19089.626799	30.057408
409.662458	19115.507707	30.062426
410.249179	19146.562622	30.067444
410.644540	19187.843037	30.072461
410.834575	19222.947608	30.077479
411.178693	19246.768782	30.082496
411.471065	19271.151915	30.087514
412.218505	19298.461487	30.092532
412.448265	19341.950028	30.097549
412.700529	19371.802637	30.102567
413.367765	19403.319243	30.107584
413.599553	19433.987269	30.112602
414.102279	19464.456012	30.117620
414.681379	19502.446500	30.122637
415.190299	19532.487097	30.127655
415.557073	19566.910447	30.132672
415.677759	19603.681099	30.137690
416.388636	19628.235130	30.142708
416.621745	19666.180771	30.147725
416.938217	19696.103736	30.152743
417.677485	19733.434461	30.157760
418.055492	19761.556376	30.162778
418.615093	19792.189727	30.167796
418.912517	19817.250747	30.172813
419.509140	19837.828944	30.177831
419.682968	19876.566855	30.182848
420.039399	19906.057904	30.187866
420.502819	19938.086953	30.192884
420.562602	19976.667389	30.197901
420.944518	20010.866845	30.202919
421.525575	20036.338467	30.207936
422.047377	20073.589270	30.212954
422.691367	20086.196516	30.217972
423.016862	20122.608052	30.222989
422.975497	20146.442271	30.228007
423.669375	20173.623396	30.233024
423.928156	20214.730288	30.238042
424.594335	20245.999550	30.243060
425.312296	20278.903142	30.248077
425.271137	20321.608175	30.253095
425.447661	20339.007083	30.258112
425.780799	20379.832471	30.263130
426.181522	20416.246383	30.268148
426.901251	20454.154266	30.273165
426.970587	20492.652318	30.278183
427.776095	20518.090682	30.283200
427.806654	20572.981409	30.288218
428.287439	20598.076315	30.293236
429.148457	20639.967509	30.298253
429.200276	20688.702984	30.303271
429.973607	20719.110305	30.308288
430.100666	20769.263595	30.313306
430.828066	20797.813462	30.318324
431.288324	20839.637456	30.323341
431.554376	20885.254071	30.328359
432.459325	20901.052515	30.333376
432.407715	20946.643031	30.338394
432.872251	20982.792186	30.343412
433.298260	21013.372614	30.348429
433.685461	21054.958539	30.353447
434.183038	21095.883007	30.358464
434.732916	21137.815893	30.363482
435.261251	21175.304560	30.368500
435.667478	21217.964628	30.373517
436.084187	21250.817488	30.378535
436.787315	21285.811497	30.383552
436.676397	21329.019403	30.388570
437.314408	21355.730786	30.393588
437.755765	21404.799621	30.398605
438.206360	21447.867606	30.403623
438.738037	21483.508476	30.408640
439.366775	21525.878645	30.413658
439.558013	21559.857369	30.418676
440.206595	21599.343731	30.423693
440.484996	21637.464488	30.428711
441.023227	21666.223728	30.433728
441.484607	21708.790763	30.438746
441.940187	21739.526867	30.443764
442.370270	21780.759018	30.448781
442.373453	21825.658518	30.453799
443.343278	21863.635405	30.458816
443.767234	21895.930145	30.463834
444.372301	21935.189554	30.468852
444.786523	21971.686582	30.473869
444.918398	22001.454976	30.478887
445.434849	22040.694605	30.483904
445.581257	22091.928712	30.488922
446.148693	22126.984762	30.493940
446.596903	22157.235614	30.498957
447.067172	22210.661845	30.503975
447.605708	22245.066972	30.508992
447.682553	22299.384833	30.514010
448.281740	22325.033521	30.519028
448.834612	22369.700006	30.524045
449.089518	22415.464502	30.529063
449.711954	22452.418501	30.534080
449.807321	22494.822593	30.539098
450.573739	22544.807534	30.544116
451.101529	22580.006689	30.549133
451.343481	22622.221274	30.554151
451.955260	22647.677570	30.559168
452.326320	22695.404113	30.564186
452.801502	22734.697906	30.569204
453.175703	22756.245246	30.574221
453.801422	22800.560209	30.579239
454.467979	22834.805008	30.584256
454.495263	22871.650260	30.589274
454.856981	22918.672541	30.594292
455.246009	22959.649437	30.599309
455.782958	23007.374634	30.604327
456.113737	23035.246479	30.609344
456.628725	23095.945389	30.614362
456.741732	23135.132890	30.619380
457.647875	23175.397132	30.624397
458.002792	23224.420881	30.629415
458.588871	23266.310467	30.634432
459.045410	23305.421013	30.639450
459.305088	23343.823078	30.644468
460.038312	23387.412172	30.649485
460.363379	23434.025636	30.654503
461.350049	23475.423681	30.659520
461.493603	23515.819652	30.664538
461.638780	23563.669584	30.669556
462.850586	23610.281871	30.674573
462.611506	23648.756118	30.679591
463.432482	23693.558330	30.684608
463.629842	23736.853796	30.689626
463.989407	23783.014653	30.694644
464.804571	23823.681836	30.699661
465.340954	23875.992180	30.704679
465.604981	23918.375056	30.709696
466.178755	23967.279566	30.714714
466.709384	24008.010043	30.719732
467.382524	24038.438335	30.724749
467.476981	24100.148703	30.729767
468.274459	24136.621648	30.734784
468.747605	24172.517548	30.739802
469.086740	24218.471645	30.744820
469.873464	24257.659047	30.749837
469.807194	24312.502172	30.754855
470.978200	24350.512839	30.759872
471.055818	24385.295040	30.764890
471.366814	24427.201456	30.769908
471.961072	24474.044456	30.774925
472.248907	24510.110505	30.779943
472.691528	24555.978994	30.784960
473.206072	24596.328742	30.789978
473.795339	24653.783269	30.794996
474.373095	24687.426713	30.800013
474.715918	24736.125621	30.805031
475.219445	24781.984637	30.810048
475.526157	24827.677635	30.815066
476.137645	24879.619052	30.820084
476.459085	24927.303268	30.825101
476.975636	24973.905010	30.830119
477.351307	25018.896355	30.835136
478.216321	25061.851284	30.840154
478.757376	25103.954690	30.845172
478.997038	25143.792929	30.850189
479.435295	25191.985291	30.855207
479.996915	25238.435203	30.860224
480.067382	25281.023800	30.865242
480.770006	25321.072871	30.870260
481.516301	25367.555656	30.875277
481.718583	25423.420846	30.880295
482.120810	25468.809558	30.885312
482.703962	25508.396242	30.890330
483.081506	25558.725617	30.895348
483.742964	25590.167952	30.900365
483.806219	25642.246552	30.905383
484.677383	25688.409890	30.910400
485.132531	25720.949583	30.915418
485.510995	25764.936212	30.920436
485.944060	25800.075665	30.925453
486.262432	25856.598062	30.930471
487.038536	25896.175790	30.935488
487.697070	25934.151759	30.940506
487.951857	25983.237817	30.945524
488.628607	26023.365355	30.950541
488.737444	26079.945237	30.955559
489.030997	26120.669489	30.960576
489.779764	26172.582631	30.965594
490.211613	26223.974281	30.970612
490.575492	26266.892127	30.975629
491.391696	26319.144685	30.980647
491.637965	26363.075854	30.985664
492.115753	26420.191973	30.990682
492.839380	26463.202188	30.995700
493.939590	26514.701761	31.000717
494.159339	26559.640916	31.005735
494.302243	26606.510785	31.010752
495.245500	26656.273436	31.015770
495.447488	26705.417597	31.020788
496.108421	26746.849060	31.025805
496.560482	26788.592776	31.030823
496.957592	26838.275983	31.035840
497.686969	26880.444047	31.040858
497.981736	26936.787768	31.045876
498.718994	26967.021375	31.050893
499.062644	27019.029332	31.055911
499.479817	27061.192717	31.060928
500.265046	27109.430810	31.065946
500.363113	27166.672160	31.070964
501.100544	27207.215114	31.075981
501.390868	27251.750070	31.080999
502.023092	27305.692181	31.086016
502.595674	27351.010331	31.091034
503.079465	27410.598734	31.096052
503.923149	27446.582103	31.101069
504.322365	27501.579149	31.106087
504.677472	27539.126205	31.111104
505.292621	27583.295959	31.116122
505.644907	27636.796460	31.121140
506.601845	27677.446149	31.126157
506.929885	27718.269399	31.131175
507.195194	27763.298771	31.136192
507.723298	27812.862144	31.141210
508.409987	27856.771541	31.146228
508.649282	27904.755172	31.151245
509.399059	27966.314134	31.156263
509.719289	28009.382321	31.161280
510.368511	28053.295260	31.166298
510.520077	28107.379333	31.171316
511.392023	28145.542518	31.176333
512.181055	28206.341864	31.181351
512.440935	28253.852999	31.186368
513.589658	28277.635677	31.191386
513.913074	28319.088889	31.196404
514.249510	28358.729230	31.201421
514.714163	28398.108685	31.206439
514.910981	28449.530044	31.211456
515.738727	28492.483901	31.216474
516.055259	28537.497335	31.221492
516.340754	28575.316835	31.226509
516.810405	28614.490892	31.231527
517.175432	28659.603878	31.236544
518.114978	28698.239774	31.241562
518.461675	28747.299509	31.246580
518.979092	28787.522910	31.251597
519.455394	28840.782595	31.256615
520.220916	28880.163833	31.261632
520.584908	28917.100354	31.266650
520.868988	28976.111967	31.271668
521.532635	29003.036101	31.276685
522.001421	29058.578648	31.281703
522.554488	29112.943280	31.286720
523.056464	29148.112817	31.291738
523.328453	29200.817445	31.296756
523.840978	29240.960672	31.301773
524.628741	29295.940102	31.306791
524.737861	29346.861206	31.311808
525.254335	29400.062314	31.316826
525.670078	29451.216929	31.321844
526.503970	29506.375528	31.326861
527.099110	29562.756910	31.331879
527.699011	29616.727299	31.336896
528.349487	29660.612527	31.341914
528.425772	29720.979806	31.346932
529.065939	29773.290808	31.351949
529.636348	29827.970289	31.356967
530.084598	29883.954239	31.361984
530.694775	29932.449968	31.367002
530.984163	30001.203681	31.372020
531.537311	30038.057632	31.377037
532.327443	30101.983718	31.382055
532.691873	30160.373942	31.387072
533.237941	30211.644877	31.392090
533.647913	30277.814653	31.397108
534.665972	30329.446391	31.402125
535.165038	30387.638407	31.407143
535.729060	30443.071772	31.412160
536.517954	30497.707722	31.417178
536.497646	30554.074225	31.422196
537.414012	30603.691696	31.427213
537.974705	30658.741364	31.432231
538.181826	30723.075378	31.437248
538.869858	30767.550327	31.442266
539.323963	30821.103661	31.447284
539.945181	30884.596730	31.452301
540.927855	30936.794575	31.457319
541.004276	30994.250797	31.462336
541.914093	31039.753041	31.467354
542.411097	31096.947539	31.472372
542.901381	31146.889459	31.477389
543.733171	31193.373666	31.482407
544.027604	31264.441107	31.487424
544.839711	31301.567228	31.492442
545.519586	31353.485107	31.497460
545.772442	31397.970546	31.502477
546.448249	31454.619154	31.507495
546.741236	31501.811760	31.512512
547.063745	31551.624818	31.517530
547.252172	31610.550657	31.522548
548.062068	31669.127749	31.527565
549.048613	31729.133572	31.532583
549.478521	31783.880234	31.537600
549.950718	31827.027303	31.542618
550.899287	31875.961471	31.547636
551.238112	31921.544689	31.552653
551.540413	31971.116153	31.557671
552.273149	32028.893116	31.562688
552.812158	32075.286095	31.567706
553.724424	32119.260352	31.572724
554.176305	32174.010895	31.577741
554.772599	32212.487292	31.582759
555.128796	32264.237364	31.587776
555.677764	32297.316526	31.592794
556.050193	32351.033157	31.597812
556.491320	32394.410785	31.602829
557.245031	32447.159007	31.607847
557.625609	32502.133776	31.612864
558.060779	32532.786715	31.617882
558.291182	32603.005515	31.622900
558.822278	32662.540803	31.627917
559.760593	32713.012555	31.632935
559.976984	32777.109519	31.637952
560.448370	32830.492518	31.642970
560.950837	32882.860762	31.647988
561.534094	32951.208119	31.653005
562.068933	33007.007768	31.658023
562.186681	33074.823597	31.663040
563.103426	33144.729017	31.668058
563.780809	33205.822867	31.673076
564.611688	33270.974885	31.678093
565.475753	33327.446856	31.683111
565.521031	33398.677662	31.688128
566.534428	33448.722537	31.693146
567.344240	33512.856499	31.698164
567.640583	33567.346744	31.703181
568.384776	33615.398072	31.708199
569.002563	33684.588247	31.713216
569.466270	33737.009594	31.718234
570.389132	33789.232053	31.723252
570.695005	33847.530505	31.728269
571.398988	33893.490689	31.733287
571.641051	33951.358237	31.738304
572.314142	34004.932280	31.743322
573.401987	34061.438976	31.748340
573.521882	34109.699067	31.753357
574.262859	34172.745429	31.758375
574.527401	34241.040005	31.763392
575.491170	34299.966377	31.768410
575.810711	34355.171548	31.773428
576.073192	34413.472710	31.778445
576.670295	34469.250847	31.783463
577.415738	34536.753769	31.788480
577.929830	34595.752358	31.793498
578.820955	34660.135762	31.798516
579.176662	34717.996449	31.803533
579.753109	34777.247255	31.808551
580.499943	34840.105644	31.813568
581.351799	34891.847599	31.818586
582.159367	34948.299325	31.823604
582.462976	35004.945066	31.828621
583.651941	35050.111588	31.833639
583.656725	35107.668660	31.838656
584.488930	35162.810429	31.843674
584.892671	35214.794720	31.848692
585.344474	35275.724667	31.853709
585.938628	35330.903182	31.858727
586.368081	35385.219129	31.863744
586.968998	35437.837354	31.868762
587.451731	35499.914878	31.873780
588.160594	35564.356927	31.878797
588.544883	35620.868173	31.883815
589.374774	35682.115663	31.888832
589.962219	35732.922261	31.893850
590.529923	35793.481307	31.898868
591.033104	35854.196410	31.903885
591.946017	35895.601367	31.908903
592.284388	35958.013648	31.913920
592.625017	36015.246627	31.918938
593.213808	36054.590995	31.923956
593.749766	36114.304224	31.928973
594.197955	36171.788172	31.933991
594.738017	36236.008060	31.939008
595.318376	36301.742768	31.944026
595.786388	36354.161569	31.949044
596.536805	36423.229882	31.954061
597.278551	36479.356434	31.959079
597.774024	36555.145888	31.964096
598.163397	36620.632452	31.969114
599.092029	36669.488364	31.974132
599.125899	36740.109353	31.979149
600.024908	36797.852107	31.984167
600.421280	36878.668241	31.989184
601.212024	36936.754442	31.994202
601.921385	37003.098447	31.999220
602.237875	37074.374668	32.004237
603.129547	37129.818771	32.009255
603.609831	37207.207386	32.014272
604.322491	37265.689472	32.019290
604.684334	37336.428958	32.024308
605.240940	37403.484621	32.029325
605.922487	37473.272192	32.034343
606.970773	37549.580357	32.039360
607.422375	37608.993676	32.044378
608.300131	37676.606393	32.049396
608.603709	37740.422527	32.054413
609.633234	37803.575881	32.059431
610.301748	37874.576049	32.064448
611.229645	37929.773559	32.069466
611.852224	37990.845366	32.074484
612.254456	38062.351161	32.079501
612.641689	38124.737557	32.084519
613.020760	38185.408399	32.089536
613.603254	38249.934567	32.094554
614.472822	38317.841417	32.099572
614.545944	38385.015404	32.104589
615.779540	38453.342321	32.109607
616.207957	38520.079243	32.114624
616.609556	38587.761492	32.119642
617.631036	38654.059880	32.124660
618.259269	38728.851582	32.129677
618.893094	38794.371811	32.134695
619.483770	38859.337543	32.139712
620.470287	38923.906575	32.144730
621.385991	38982.464749	32.149748
621.530634	39048.988549	32.154765
622.259917	39113.136784	32.159783
622.821986	39164.970459	32.164800
623.158596	39236.561148	32.169818
624.253017	39298.039074	32.174836
624.360697	39365.517135	32.179853
625.158471	39428.821783	32.184871
625.739166	39495.022526	32.189888
626.052041	39558.571991	32.194906
627.096399	39624.712278	32.199924
627.435678	39696.275907	32.204941
628.134540	39754.222137	32.209959
628.843012	39829.462783	32.214976
629.345953	39898.256907	32.219994
629.844130	39960.987917	32.225012
630.578435	40040.474167	32.230029
631.382441	40101.586139	32.235047
631.957586	40179.593530	32.240064
632.312388	40249.101658	32.245082
633.210831	40306.549402	32.250100
633.745586	40367.176452	32.255117
634.141288	40429.780798	32.260135
634.793549	40488.756716	32.265152
634.843333	40557.700880	32.270170
636.186995	40623.400635	32.275188
636.399884	40698.269070	32.280205
637.070981	40768.572877	32.285223
637.785783	40837.647993	32.290240
638.347095	40902.237502	32.295258
638.716913	40964.383874	32.300276
639.405890	41048.749977	32.305293
640.050235	41118.952207	32.310311
640.595523	41195.510311	32.315328
641.080765	41268.612284	32.320346
642.212294	41341.762321	32.325364
642.481558	41427.746522	32.330381
643.284762	41504.253763	32.335399
643.838701	41569.481385	32.340416
644.624521	41653.771084	32.345434
645.717866	41734.392283	32.350452
645.854990	41819.715076	32.355469
646.184790	41896.744246	32.360487
647.233464	41973.515897	32.365504
647.956411	42054.171349	32.370522
649.084381	42127.666048	32.375540
649.547461	42206.537168	32.380557
650.239226	42282.911356	32.385575
650.774772	42348.195272	32.390592
651.118357	42436.208224	32.395610
651.513188	42515.890715	32.400628
652.199610	42593.971955	32.405645
653.170096	42684.581793	32.410663
654.034851	42763.960283	32.415680
654.892546	42842.197350	32.420698
655.803285	42906.022486	32.425716
656.366912	42988.337496	32.430733
656.988703	43056.163870	32.435751
657.744326	43128.840081	32.440768
658.532542	43205.606231	32.445786
659.202662	43274.817785	32.450804
659.755808	43357.985481	32.455821
660.048243	43429.564954	32.460839
660.809461	43508.354368	32.465856
661.243793	43587.937020	32.470874
662.317379	43662.015102	32.475892
663.030533	43737.927571	32.480909
663.575318	43819.055853	32.485927
664.356921	43882.514169	32.490944
664.811329	43966.913360	32.495962
665.538823	44039.686173	32.500980
666.196476	44129.754855	32.505997
666.808163	44199.503635	32.511015
667.670787	44269.899499	32.516032
668.048107	44349.927394	32.521050
668.906235	44429.067762	32.526068
669.585761	44518.035868	32.531085
670.031734	44592.827704	32.536103
670.863109	44661.929293	32.541120
671.586493	44748.336760	32.546138
672.364013	44822.525243	32.551156
672.690286	44899.229499	32.556173
673.196363	44981.745921	32.561191
674.669278	45060.228344	32.566208
674.611473	45135.326708	32.571226
675.252111	45220.657484	32.576244
676.074306	45297.148697	32.581261
677.057094	45378.953304	32.586279
677.717235	45451.401691	32.591296
678.154423	45537.140162	32.596314
678.764488	45603.335668	32.601332
679.116598	45667.651017	32.606349
679.880413	45748.574548	32.611367
681.129857	45815.119743	32.616384
681.539644	45904.445314	32.621402
682.240450	45961.418990	32.626420
683.076915	46036.837191	32.631437
683.428439	46114.704273	32.636455
684.343421	46193.327919	32.641472
684.937111	46263.077837	32.646490
685.456089	46338.600285	32.651508
686.147617	46415.420792	32.656525
686.519401	46505.832314	32.661543
687.254182	46570.441106	32.666560
687.765772	46666.296567	32.671578
688.626345	46752.466289	32.676596
689.652241	46842.408046	32.681613
690.220071	46924.313239	32.686631
691.093340	47002.473447	32.691648
691.655329	47094.678446	32.696666
692.173678	47177.113979	32.701684
693.157415	47259.558148	32.706701
693.692813	47359.240659	32.711719
694.327103	47426.774361	32.716736
695.086803	47525.896405	32.721754
695.760069	47610.117743	32.726772
696.392532	47689.719627	32.731789
696.779189	47790.300621	32.736807
697.652152	47869.623455	32.741824
698.527231	47965.441111	32.746842
699.153528	48050.720657	32.751860
699.746126	48147.833418	32.756877
700.385721	48246.915907	32.761895
701.388215	48326.800313	32.766912
701.924945	48428.354662	32.771930
702.938596	48509.122278	32.776948
703.672623	48606.217125	32.781965
704.273618	48689.514020	32.786983
705.112674	48773.839386	32.792000
705.612185	48867.114965	32.797018
706.182070	48960.249866	32.802036
706.722729	49051.394009	32.807053
707.679332	49143.546763	32.812071
708.448191	49226.492913	32.817088
709.215185	49328.282386	32.822106
709.751524	49418.462531	32.827124
710.975415	49503.908667	32.832141
711.563226	49601.620186	32.837159
712.678597	49686.415506	32.842176
713.163547	49782.736312	32.847194
713.746489	49859.335943	32.852212
714.298153	49950.981554	32.857229
715.063116	50048.369138	32.862247
716.202431	50130.070317	32.867264
716.751874	50222.213463	32.872282
717.294936	50305.451127	32.877300
718.096070	50390.813201	32.882317
718.417145	50477.474254	32.887335
719.099865	50568.030369	32.892352
719.643229	50671.642179	32.897370
720.559081	50762.084832	32.902388
721.320267	50863.482219	32.907405
721.899056	50945.781781	32.912423
722.712979	51044.151762	32.917440
723.219442	51138.517409	32.922458
723.676479	51245.797949	32.927476
724.545448	51329.643099	32.932493
725.443566	51424.419149	32.937511
726.337147	51502.537441	32.942528
726.861415	51605.658319	32.947546
728.011773	51691.258950	32.952564
728.461284	51772.970606	32.957581
729.203115	51860.673788	32.962599
729.963098	51946.024238	32.967616
730.308231	52026.383316	32.972634
730.881226	52122.960194	32.977652
731.821086	52219.249431	32.982669
732.382759	52327.864273	32.987687
733.365182	52407.885751	32.992704
733.880578	52517.280059	32.997722
734.753080	52609.633787	33.002740
735.132759	52709.739258	33.007757
735.849307	52815.620861	33.012775
736.666042	52915.610864	33.017792
737.539584	53014.581120	33.022810
738.290016	53123.914665	33.027828
739.137923	53217.696861	33.032845
739.995797	53323.450425	33.037863
740.581427	53422.723084	33.042880
741.325819	53522.172161	33.047898
742.216165	53630.158593	33.052916
743.225373	53719.342216	33.057933
743.461952	53825.365521	33.062951
744.493596	53926.373935	33.067968
745.499798	54037.913210	33.072986
746.150875	54132.875926	33.078004
747.153582	54228.905589	33.083021
747.846465	54335.494305	33.088039
748.487192	54421.165898	33.093056
749.027251	54519.383824	33.098074
749.963788	54625.523109	33.103092
750.745555	54727.518402	33.108109
751.392917	54826.061298	33.113127
751.991833	54917.605491	33.118144
752.945432	55028.034371	33.123162
753.884059	55125.279512	33.128180
755.060982	55227.957611	33.133197
755.332578	55331.733785	33.138215
756.496293	55422.245414	33.143232
757.065754	55534.743670	33.148250
757.621445	55625.502128	33.153268
758.864591	55724.633366	33.158285
759.491253	55828.966325	33.163303
760.314891	55923.018138	33.168320
760.953388	56021.119802	33.173338
761.544384	56116.714896	33.178356
762.193221	56216.458718	33.183373
763.029763	56319.173487	33.188391
763.780020	56414.231831	33.193408
764.552341	56517.672288	33.198426
765.190710	56627.050052	33.203444
765.989668	56722.822181	33.208461
766.603671	56832.925476	33.213479
767.507960	56935.550063	33.218496
768.468368	57038.854684	33.223514
769.034956	57142.161787	33.228532
769.921602	57245.429121	33.233549
770.547113	57350.136739	33.238567
771.361802	57443.742212	33.243584
772.297388	57552.014230	33.248602
772.911768	57659.183520	33.253620
773.949374	57747.615903	33.258637
774.271737	57862.961313	33.263655
775.346221	57959.610101	33.268672
776.208977	58063.568101	33.273690
776.867410	58160.084445	33.278708
777.840061	58242.045928	33.283725
778.123139	58344.357066	33.288743
779.325555	58435.444716	33.293760
780.082508	58528.812011	33.298778
780.483659	58632.457483	33.303796
781.252117	58711.124187	33.308813
781.820223	58817.814364	33.313831
782.954612	58912.050004	33.318848
783.993842	59011.743155	33.323866
784.444711	59110.725179	33.328884
785.458716	59197.227653	33.333901
786.130254	59305.830850	33.338919
786.852421	59401.009096	33.343936
787.987999	59505.675153	33.348954
788.301175	59601.667741	33.353972
789.403151	59702.150234	33.358989
789.991354	59814.486101	33.364007
790.770921	59916.767313	33.369024
791.381700	60026.787476	33.374042
792.205001	60124.657393	33.379060
792.593315	60235.789905	33.384077
793.406825	60348.824598	33.389095
794.330379	60471.208306	33.394112
795.006101	60577.219996	33.399130
795.671830	60708.148535	33.404148
796.576972	60815.273813	33.409165
797.473906	60935.882378	33.414183
798.051311	61051.172151	33.419200
799.182024	61161.573837	33.424218
799.820116	61285.058838	33.429236
800.794344	61399.298945	33.434253
801.429717	61520.826456	33.439271
802.390735	61640.998785	33.444288
803.291023	61753.856248	33.449306
803.997344	61867.081410	33.454324
805.332147	61984.286423	33.459341
805.818264	62098.061258	33.464359
806.335661	62212.191833	33.469376
807.401056	62325.037772	33.474394
808.361367	62439.127955	33.479412
809.198615	62559.749631	33.484429
810.194238	62674.031224	33.489447
810.898375	62787.893912	33.494464
811.836764	62903.987718	33.499482
812.364896	63022.716367	33.504500
813.466708	63128.519071	33.509517
813.953041	63253.065007	33.514535
814.741760	63365.064810	33.519552
815.776923	63475.734942	33.524570
816.498215	63605.787801	33.529588
817.337859	63718.362644	33.534605
817.951772	63837.745514	33.539623
819.192745	63960.457831	33.544640
820.048945	64073.929494	33.549658
820.492807	64201.648830	33.554676
821.779995	64312.698963	33.559693
823.225439	64420.499578	33.564711
823.351033	64534.827884	33.569728
824.241611	64642.399024	33.574746
825.108313	64748.495428	33.579764
825.965506	64861.155746	33.584781
826.691526	64978.352003	33.589799
827.416482	65085.788465	33.594816
828.530481	65184.506754	33.599834
829.103378	65295.117640	33.604852
829.806168	65416.125869	33.609869
830.540959	65539.291557	33.614887
831.557474	65630.144810	33.619904
832.635226	65728.062473	33.624922
833.207915	65846.705055	33.629940
833.465096	65967.442467	33.634957
834.778366	66059.329553	33.639975
835.293290	66165.990770	33.644992
835.976891	66284.547943	33.650010
836.575619	66396.930539	33.655028
838.015365	66503.958926	33.660045
838.608941	66631.213159	33.665063
839.013033	66753.416488	33.670080
840.226986	66866.205613	33.675098
841.519839	66978.697795	33.680116
842.125235	67094.313667	33.685133
842.373779	67218.069079	33.690151
843.206438	67346.097341	33.695168
844.452011	67460.869632	33.700186
845.175750	67598.489499	33.705204
845.991769	67721.142420	33.710221
847.068597	67842.570613	33.715239
847.624779	67961.790539	33.720256
848.860270	68084.521608	33.725274
848.989732	68229.900473	33.730292
849.967526	68342.907253	33.735309
850.989876	68465.985589	33.740327
851.796451	68594.341845	33.745344
852.762609	68730.936305	33.750362
853.818391	68857.400371	33.755380
855.004475	68982.142800	33.760397
855.354871	69106.442468	33.765415
856.090877	69246.233402	33.770432
857.698786	69362.081534	33.775450
858.614423	69497.867287	33.780468
859.389399	69615.662919	33.785485
860.130212	69743.714500	33.790503
861.344169	69865.567856	33.795520
862.534436	69984.061929	33.800538
862.910562	70111.720760	33.805556
863.815811	70235.726565	33.810573
864.939974	70350.142494	33.815591
865.447692	70481.189977	33.820608
866.453232	70604.972662	33.825626
867.602399	70728.896715	33.830644
868.462746	70849.890941	33.835661
869.232005	70969.775346	33.840679
869.713175	71102.841849	33.845696
870.589902	71222.760476	33.850714
871.430610	71347.972185	33.855732
872.481352	71478.183432	33.860749
873.421633	71600.572482	33.865767
873.821560	71737.899463	33.870784
874.805837	71860.883456	33.875802
875.900450	71992.064389	33.880820
876.690415	72114.057517	33.885837
877.810474	72237.881225	33.890855
878.533744	72369.973245	33.895872
879.612847	72499.768579	33.900890
880.390674	72632.087154	33.905908
881.662947	72752.391517	33.910925
882.349978	72879.066701	33.915943
883.481371	73006.541846	33.920960
884.387175	73126.048820	33.925978
885.054454	73243.717647	33.930996
885.816576	73374.386428	33.936013
886.727170	73493.711226	33.941031
887.653324	73625.536997	33.946048
888.615561	73739.491696	33.951066
889.239935	73857.272114	33.956084
890.241374	73972.682447	33.961101
891.451256	74083.119632	33.966119
891.702861	74206.718698	33.971136
892.721871	74325.669619	33.976154
893.479588	74439.427784	33.981172
894.395897	74559.301348	33.986189
895.470879	74672.989283	33.991207
896.176649	74802.392036	33.996224
897.009395	74920.889999	34.001242
897.714132	75059.325893	34.006260
898.503660	75181.114866	34.011277
899.678183	75301.860522	34.016295
900.385906	75433.145082	34.021312
901.509399	75559.567518	34.026330
902.040053	75693.020666	34.031348
902.876161	75818.018435	34.036365
903.846731	75957.491219	34.041383
904.771982	76090.527318	34.046400
905.868093	76218.646796	34.051418
906.434346	76356.063779	34.056436
907.407769	76497.822803	34.061453
908.296291	76633.233783	34.066471
909.200250	76774.202779	34.071488
910.068177	76915.102727	34.076506
911.140922	77051.668588	34.081524
912.330315	77184.503106	34.086541
913.335062	77326.799877	34.091559
914.425469	77464.377386	34.096576
915.481285	77599.943688	34.101594
915.850022	77732.853931	34.106612
916.890653	77868.437025	34.111629
918.136400	78005.422892	34.116647
918.636723	78144.683527	34.121664
919.767733	78283.973567	34.126682
921.031333	78422.325343	34.131700
921.764461	78557.767368	34.136717
923.031737	78691.616382	34.141735
923.959055	78827.635181	34.146752
925.216900	78958.324514	34.151770
926.289798	79080.391590	34.156788
926.707956	79215.592353	34.161805
927.958709	79346.158596	34.166823
928.929416	79485.672366	34.171840
930.149114	79604.630994	34.176858
931.122501	79729.121872	34.181876
931.673400	79851.633694	34.186893
932.623656	79977.192522	34.191911
933.407234	80122.953285	34.196928
934.344539	80238.084093	34.201946
935.282911	80379.430627	34.206964
936.315591	80515.878671	34.211981
937.089950	80644.127256	34.216999
938.035199	80781.654152	34.222016
939.048165	80912.161204	34.227034
939.979345	81047.129904	34.232052
940.627044	81178.495996	34.237069
941.704954	81306.685465	34.242087
942.321070	81447.029094	34.247104
943.160520	81587.754198	34.252122
944.255171	81730.215706	34.257140
945.269836	81871.603169	34.262157
946.521431	82000.723116	34.267175
947.403153	82146.233859	34.272192
948.132453	82283.748574	34.277210
949.200027	82418.778739	34.282228
950.392005	82568.517678	34.287245
951.061301	82698.984207	34.292263
951.885708	82836.998972	34.297280
952.431821	82969.853619	34.302298
953.616182	83094.365939	34.307316
954.385807	83228.804791	34.312333
955.290633	83348.682818	34.317351
956.339632	83490.365602	34.322368
957.106088	83623.693734	34.327386
958.162556	83762.257745	34.332404
959.036329	83899.549421	34.337421
960.158527	84033.567684	34.342439
960.973849	84181.576153	34.347456
961.969162	84322.867975	34.352474
962.896343	84456.256574	34.357492
963.987545	84594.699601	34.362509
964.966197	84738.331462	34.367527
966.106884	84879.286264	34.372544
966.992049	85022.163400	34.377562
967.950930	85161.378308	34.382580
969.030975	85307.319069	34.387597
970.055297	85443.392753	34.392615
970.838725	85597.869534	34.397632
971.592408	85744.170711	34.402650
972.778428	85881.713513	34.407668
973.550394	86041.548268	34.412685
974.665706	86179.186768	34.417703
975.563885	86336.028649	34.422720
976.604024	86479.642058	34.427738
977.649669	86630.804503	34.432756
978.681010	86784.001521	34.437773
979.486572	86928.751177	34.442791
980.540487	87090.109425	34.447808
981.458015	87241.347594	34.452826
983.049631	87388.748073	34.457844
983.671678	87548.048322	34.462861
984.558865	87698.288273	34.467879
985.877371	87838.402461	34.472896
986.320651	87996.855678	34.477914
987.261517	88157.221061	34.482932
988.351730	88317.322358	34.487949
989.732533	88465.276985	34.492967
990.928440	88620.458420	34.497984
991.396266	88781.127720	34.503002
992.888413	88929.573093	34.508020
993.412452	89093.949985	34.513037
994.360766	89246.467854	34.518055
995.891923	89406.351674	34.523072
996.629896	89558.608872	34.528090
997.770798	89716.046844	34.533108
998.704195	89875.728864	34.538125
999.738915	90029.003199	34.543143
1000.751374	90190.509566	34.548160
1001.861088	90342.792547	34.553178
1003.022627	90484.663330	34.558196
1003.534106	90637.249613	34.563213
1005.048619	90795.942959	34.568231
1005.926644	90943.097327	34.573248
1006.780214	91111.110651	34.578266
1007.958985	91259.096946	34.583284
1008.565772	91418.906488	34.588301
1010.255940	91579.848077	34.593319
1010.956899	91733.593492	34.598336
1012.081495	91893.763587	34.603354
1013.140175	92037.749126	34.608372
1014.031255	92194.155944	34.613389
1014.946398	92344.433014	34.618407
1016.093996	92497.071399	34.623424
1017.101399	92657.265898	34.628442
1018.143894	92810.265410	34.633460
1018.989838	92969.729123	34.638477
1020.279647	93102.758070	34.643495
1021.192173	93252.806972	34.648512
1021.728766	93394.639855	34.653530
1023.187714	93534.795615	34.658548
1024.137838	93683.018004	34.663565
1024.798100	93827.212891	34.668583
1026.148642	93962.717704	34.673600
1027.135726	94117.222025	34.678618
1028.080612	94271.493759	34.683636
1028.595803	94426.299584	34.688653
1029.723047	94574.479067	34.693671
1030.971621	94725.437206	34.698688
1031.900832	94885.285703	34.703706
1032.903546	95041.356726	34.708724
1033.727327	95211.586985	34.713741
1034.904140	95370.321566	34.718759
1035.923703	95534.109287	34.723776
1036.867969	95697.429444	34.728794
1038.188640	95860.384588	34.733812
1039.147559	96027.198767	34.738829
1040.337552	96176.137078	34.743847
1041.152571	96342.217521	34.748864
1042.023068	96514.987438	34.753882
1043.033876	96676.150675	34.758900
1044.382693	96856.073206	34.763917
1045.236807	97024.411692	34.768935
1046.552252	97197.644515	34.773952
1047.307799	97368.521166	34.778970
1048.452097	97526.458187	34.783988
1049.870435	97711.762731	34.789005
1050.784735	97875.773113	34.794023
1051.983658	98042.453401	34.799040
1052.939193	98222.476061	34.804058
1054.178456	98386.632290	34.809076
1055.070542	98556.418172	34.814093
1056.433907	98722.088136	34.819111
1057.635694	98882.892054	34.824128
1058.672318	99061.026970	34.829146
1059.519963	99214.503241	34.834164
1060.515901	99392.761169	34.839181
1061.722908	99552.124968	34.844199
1063.134450	99730.747066	34.849216
1063.668975	99902.038233	34.854234
1064.993923	100067.697992	34.859252
1066.063874	100228.798121	34.864269
1066.975808	100396.547983	34.869287
1068.252680	100573.146877	34.874304
1068.990451	100753.641313	34.879322
1070.432607	100908.048828	34.884340
1071.418121	101085.364223	34.889357
1072.306798	101259.113184	34.894375
1073.505632	101434.135344	34.899392
1074.510963	101619.251676	34.904410
1075.773759	101781.488348	34.909428
1076.497999	101958.308415	34.914445
1077.770987	102122.299431	34.919463
1078.744190	102301.170164	34.924480
1079.717346	102480.282748	34.929498
1080.872569	102645.398287	34.934516
1081.653148	102821.721036	34.939533
1082.871118	103004.538937	34.944551
1084.076709	103174.911393	34.949568
1085.261829	103357.293958	34.954586
1086.342579	103524.966548	34.959604
1087.466629	103708.260820	34.964621
1088.313052	103890.969055	34.969639
1089.619191	104059.215696	34.974656
1090.709760	104235.173787	34.979674
1092.066220	104399.196987	34.984692
1093.136958	104564.218303	34.989709
1093.732619	104731.902818	34.994727
1095.427899	104893.112153	34.999744
1096.306250	105056.889207	35.004762
1097.271168	105204.922982	35.009780
1098.273791	105382.917021	35.014797
1099.085555	105553.306690	35.019815
1100.395460	105708.125457	35.024832
1101.034385	105882.940671	35.029850
1102.301077	106062.326801	35.034868
1103.395158	106239.285564	35.039885
1104.167398	106420.567026	35.044903
1105.642004	106602.164236	35.049920
1106.539428	106780.640995	35.054938
1107.930297	106966.345578	35.059956
1109.067741	107140.352001	35.064973
1109.985175	107329.797839	35.069991
1111.081263	107507.334644	35.075008
1112.078464	107700.430425	35.080026
1112.995950	107878.670521	35.085044
1114.082731	108070.424186	35.090061
1114.974512	108269.570683	35.095079
1116.693165	108461.944660	35.100096
1117.595298	108648.400329	35.105114
1118.375106	108848.114268	35.110132
1119.875933	109050.155183	35.115149
1120.920538	109240.391429	35.120167
1122.241804	109430.139924	35.125184
1123.076326	109643.075052	35.130202
1124.462032	109835.957173	35.135220
1125.353513	110027.148940	35.140237
1126.489467	110227.941522	35.145255
1127.991440	110426.926955	35.150272
1129.159982	110628.705156	35.155290
1130.291546	110824.714492	35.160308
1131.676426	111016.300303	35.165325
1132.603420	111213.397657	35.170343
1134.003054	111414.611377	35.175360
1135.112181	111612.162857	35.180378
1136.272992	111801.979646	35.185396
1137.562381	111996.565069	35.190413
1138.597930	112195.095663	35.195431
1140.020885	112383.137545	35.200448
1140.934453	112578.181901	35.205466
1142.203382	112770.673172	35.210484
1143.528804	112964.448638	35.215501
1144.240521	113157.326076	35.220519
1145.790331	113354.589072	35.225536
1146.785238	113549.360734	35.230554
1148.402288	113730.285029	35.235572
1149.412763	113931.682668	35.240589
1150.418429	114133.792023	35.245607
1151.834293	114315.006734	35.250624
1152.529870	114516.828033	35.255642
1153.506638	114702.222699	35.260660
1154.858075	114908.841457	35.265677
1155.778513	115097.314058	35.270695
1156.875822	115289.660944	35.275712
1158.027777	115497.254536	35.280730
1159.446789	115701.346620	35.285748
1160.333934	115900.003984	35.290765
1161.450176	116103.300117	35.295783
1162.664709	116292.086795	35.300800
1163.796610	116505.164565	35.305818
1164.976904	116705.793653	35.310836
1166.217257	116907.934670	35.315853
1167.045759	117104.861592	35.320871
1168.122491	117295.514897	35.325888
1169.154396	117499.341717	35.330906
1170.137394	117688.796739	35.335924
1171.579642	117881.306789	35.340941
1172.435831	118089.728340	35.345959
1173.950147	118274.892627	35.350976
1174.792769	118475.387139	35.355994
1175.811585	118676.956307	35.361012
1177.342423	118878.492919	35.366029
1178.495859	119081.360454	35.371047
1179.822510	119286.215534	35.376064
1180.775563	119496.823340	35.381082
1182.304032	119698.733498	35.386100
1183.291324	119897.718639	35.391117
1184.648758	120118.071997	35.396135
1186.047647	120302.533298	35.401152
1186.904675	120513.430400	35.406170
1187.985854	120726.801035	35.411188
1189.692575	120930.008102	35.416205
1190.748189	121140.547391	35.421223
1191.800190	121338.745905	35.426240
1192.998479	121558.147903	35.431258
1193.748866	121774.013890	35.436276
1195.450047	121980.574642	35.441293
1196.413614	122194.444189	35.446311
1197.774553	122410.074469	35.451328
1198.851023	122624.118529	35.456346
1199.565252	122848.400412	35.461364
1201.269792	123061.697461	35.466381
1202.735462	123287.683346	35.471399
1203.836022	123504.796627	35.476416
1204.976810	123723.856525	35.481434
1206.233265	123946.206668	35.486452
1207.678262	124158.375773	35.491469
1208.655939	124378.139082	35.496487
1210.479075	124604.734785	35.501504
1211.650505	124817.764853	35.506522
1212.725556	125032.510651	35.511540
1214.188422	125240.349902	35.516557
1215.512390	125457.871183	35.521575
1216.654781	125669.099616	35.526592
1217.816981	125891.289473	35.531610
1218.882819	126098.541132	35.536628
1220.224340	126319.652484	35.541645
1221.546103	126535.698880	35.546663
1222.629033	126754.283172	35.551680
1223.990916	126968.450130	35.556698
1225.164531	127179.620418	35.561716
1226.363675	127390.116159	35.566733
1227.700451	127621.250788	35.571751
1228.858732	127834.494097	35.576768
1230.262017	128045.860476	35.581786
1231.254438	128265.370329	35.586804
1232.650212	128479.554796	35.591821
1233.671756	128691.673120	35.596839
1234.895701	128912.011178	35.601856
1236.545709	129125.486245	35.606874
1237.739285	129342.473317	35.611892
1239.021316	129561.285252	35.616909
1240.069509	129779.123290	35.621927
1241.295141	129993.371565	35.626944
1242.950198	130224.447456	35.631962
1243.809727	130431.204297	35.636980
1245.482949	130645.243566	35.641997
1246.302425	130853.746420	35.647015
1247.325761	131071.331250	35.652032
1248.761655	131293.083309	35.657050
1249.888277	131516.231742	35.662068
1251.038306	131718.309309	35.667085
1252.402787	131919.541394	35.672103
1253.809704	132128.716072	35.677120
1255.104493	132332.269440	35.682138
1256.100455	132532.539451	35.687156
1257.448581	132732.270771	35.692173
1258.576798	132950.535570	35.697191
1259.306929	133154.821313	35.702208
1260.916856	133360.826483	35.707226
1261.327389	133591.359045	35.712244
1262.763040	133805.572739	35.717261
1263.855661	134045.136211	35.722279
1265.252800	134270.338070	35.727296
1266.520145	134503.575247	35.732314
1267.478759	134739.666908	35.737332
1269.067320	134970.065195	35.742349
1270.261252	135212.067287	35.747367
1271.298959	135446.705659	35.752384
1272.394455	135686.876505	35.757402
1273.650036	135933.374443	35.762420
1275.374830	136179.657201	35.767437
1275.980274	136418.494368	35.772455
1277.359518	136665.040689	35.777472
1278.903058	136924.405137	35.782490
1279.949610	137175.067378	35.787508
1281.407667	137422.861459	35.792525
1282.802521	137685.527515	35.797543
1284.023083	137943.241573	35.802560
1285.479783	138191.104935	35.807578
1286.740301	138447.091878	35.812596
1288.146859	138701.826726	35.817613
1289.044117	138963.050763	35.822631
1290.673319	139209.447612	35.827648
1292.504343	139468.885545	35.832666
1293.427557	139725.419688	35.837684
1294.845060	139972.871413	35.842701
1296.106715	140227.502130	35.847719
1297.284507	140488.640739	35.852736
1298.813958	140740.263878	35.857754
1300.055962	140996.678739	35.862772
1301.487131	141247.992137	35.867789
1302.924863	141509.032095	35.872807
1304.156710	141759.634001	35.877824
1305.812497	142016.190895	35.882842
1306.765686	142281.970485	35.887860
1308.293638	142538.869361	35.892877
1309.643576	142794.366611	35.897895
1311.266401	143042.655909	35.902912
1312.433297	143291.605638	35.907930
1313.639212	143543.048847	35.912948
1315.146501	143793.594396	35.917965
1316.273755	144047.806004	35.922983
1317.436244	144308.760086	35.928000
1319.341750	144550.926199	35.933018
1320.571113	144818.809711	35.938036
1321.917797	145065.307303	35.943053
1323.482293	145313.292398	35.948071
1324.333812	145563.400764	35.953088
1325.795570	145812.294006	35.958106
1326.857647	146067.456505	35.963124
1328.310634	146319.309590	35.968141
1329.649336	146576.966375	35.973159
1331.102212	146825.855372	35.978176
1332.366837	147083.147519	35.983194
1333.684417	147348.511428	35.988212
1334.721010	147602.712362	35.993229
1336.526429	147856.927504	35.998247
1337.429280	148108.034122	36.003264
1338.937452	148354.603443	36.008282
1339.898546	148597.383873	36.013300
1341.472933	148827.660633	36.018317
1342.448283	149070.289611	36.023335
1343.819058	149322.113482	36.028352
1345.156678	149557.316888	36.033370
1346.299074	149810.855982	36.038388
1347.856431	150063.744782	36.043405
1349.040402	150322.810411	36.048423
1350.491123	150578.396506	36.053440
1352.030907	150826.105781	36.058458
1353.063514	151084.504063	36.063476
1354.500883	151340.604870	36.068493
1355.800825	151605.875184	36.073511
1356.935953	151863.323218	36.078528
1358.513922	152122.856092	36.083546
1359.427528	152393.180554	36.088564
1360.824735	152659.786631	36.093581
1362.258280	152939.123595	36.098599
1363.590457	153208.116184	36.103616
1365.131301	153477.101530	36.108634
1366.288939	153756.832484	36.113652
1367.957473	154032.447298	36.118669
1369.527077	154309.298150	36.123687
1370.355087	154590.243877	36.128704
1372.148874	154859.450671	36.133722
1373.523854	155137.290912	36.138740
1374.897473	155414.562510	36.143757
1376.533713	155693.632010	36.148775
1377.627236	155978.717198	36.153792
1379.224585	156255.095112	36.158810
1380.837663	156540.390233	36.163828
1382.247370	156806.705352	36.168845
1383.320745	157088.338651	36.173863
1384.552614	157375.022028	36.178880
1386.238159	157652.638226	36.183898
1387.525098	157950.112229	36.188916
1389.124457	158234.305286	36.193933
1390.344055	158512.080498	36.198951
1391.601403	158800.215976	36.203968
1393.221635	159078.258681	36.208986
1394.380233	159376.791909	36.214004
1395.832104	159658.063333	36.219021
1397.627537	159945.293321	36.224039
1398.860031	160237.895971	36.229056
1400.462286	160527.902241	36.234074
1401.768015	160815.358743	36.239092
1403.213285	161104.253162	36.244109
1404.248529	161393.090466	36.249127
1405.336484	161686.869004	36.254144
1407.428999	161972.630244	36.259162
1408.632710	162262.536776	36.264180
1410.434437	162554.642880	36.269197
1411.834199	162841.336460	36.274215
1413.165239	163136.721575	36.279232
1414.787983	163420.172265	36.284250
1416.304185	163693.669934	36.289268
1417.751658	163992.759202	36.294285
1419.276244	164273.947956	36.299303
1420.587003	164549.223243	36.304320
1422.191117	164829.945705	36.309338
1423.483498	165132.303919	36.314356
1424.617589	165406.954053	36.319373
1426.444101	165689.713473	36.324391
1427.648426	165984.047781	36.329408
1429.364499	166266.473893	36.334426
1430.552570	166546.629003	36.339444
1431.745494	166823.346480	36.344461
1433.348030	167089.517172	36.349479
1434.654251	167361.854385	36.354496
1436.259144	167626.835156	36.359514
1437.516951	167901.911749	36.364532
1438.810896	168169.662528	36.369549
1440.475640	168438.774798	36.374567
1441.699223	168726.754135	36.379584
1443.022765	168994.238437	36.384602
1444.383567	169268.341948	36.389620
1445.741766	169546.812668	36.394637
1447.171992	169826.161440	36.399655
1448.369067	170113.938192	36.404672
1449.821562	170403.019631	36.409690
1451.045794	170698.104733	36.414708
1452.320371	170994.947266	36.419725
1454.368747	171289.354286	36.424743
1455.719165	171594.639525	36.429760
1457.088189	171881.205961	36.434778
1458.527394	172181.911959	36.439796
1459.986007	172480.865428	36.444813
1461.490249	172792.110066	36.449831
1463.167640	173094.698729	36.454848
1464.294230	173383.801620	36.459866
1465.756742	173695.097120	36.464884
1467.398645	174000.451206	36.469901
1468.931150	174299.099275	36.474919
1470.373067	174614.160539	36.479936
1471.945784	174923.846726	36.484954
1473.276596	175230.135628	36.489972
1474.702786	175541.499756	36.494989
1476.387503	175850.399157	36.500007
1477.800186	176174.574767	36.505024
1479.300607	176486.326024	36.510042
1480.677442	176804.584895	36.515060
1482.064705	177120.318497	36.520077
1483.671400	177435.599017	36.525095
1484.851248	177757.577010	36.530112
1486.338794	178082.856794	36.535130
1488.023231	178410.289103	36.540148
1489.296471	178730.709466	36.545165
1491.095517	179057.581253	36.550183
1492.550465	179393.472469	36.555200
1494.255332	179725.402757	36.560218
1495.884036	180035.403165	36.565236
1497.158933	180365.872859	36.570253
1498.575586	180679.808635	36.575271
1500.209569	181015.033458	36.580288
1501.691297	181340.867825	36.585306
1503.674835	181658.828117	36.590324
1505.045856	181992.719120	36.595341
1506.405260	182319.531653	36.600359
1507.730067	182638.558584	36.605376
1509.216741	182960.035756	36.610394
1510.879953	183290.649912	36.615412
1512.363291	183637.047731	36.620429
1513.949640	183966.193628	36.625447
1515.436727	184310.500758	36.630464
1516.914002	184629.184173	36.635482
1518.404544	184961.626704	36.640500
1520.121681	185292.777152	36.645517
1521.780329	185623.418807	36.650535
1523.189965	185958.343177	36.655552
1524.719893	186287.258319	36.660570
1526.468310	186620.962852	36.665588
1527.492439	186952.834190	36.670605
1529.230874	187284.856012	36.675623
1530.924486	187611.390738	36.680640
1532.248279	187935.348090	36.685658
1533.961741	188255.320439	36.690676
1535.099162	188566.618145	36.695693
1536.564034	188864.572683	36.700711
1537.933717	189192.820068	36.705728
1539.655411	189504.305500	36.710746
1541.192617	189819.910625	36.715764
1542.099674	190154.053781	36.720781
1543.450444	190474.542436	36.725799
1544.812722	190810.226245	36.730816
1546.351164	191136.780797	36.735834
1548.323558	191484.668615	36.740852
1549.640608	191825.011773	36.745869
1551.448607	192156.211624	36.750887
1552.696359	192503.387108	36.755904
1554.160632	192845.907811	36.760922
1555.934419	193186.957427	36.765940
1557.211500	193551.932339	36.770957
1558.811771	193896.188260	36.775975
1560.240188	194248.624788	36.780992
1561.674452	194604.540819	36.786010
1563.278921	194970.625099	36.791028
1564.738089	195333.104576	36.796045
1566.546400	195693.624080	36.801063
1568.115926	196059.733008	36.806080
1569.798367	196426.739422	36.811098
1571.697187	196794.588145	36.816116
1573.193418	197153.973854	36.821133
1574.754148	197525.132614	36.826151
1576.258418	197894.182541	36.831168
1577.758297	198266.307652	36.836186
1579.301666	198633.844341	36.841204
1580.796334	199008.373939	36.846221
1582.574876	199378.084910	36.851239
1584.103823	199764.445836	36.856256
1585.666037	200141.484293	36.861274
1587.461872	200513.102908	36.866292
1589.139923	200887.929765	36.871309
1590.663100	201257.121532	36.876327
1592.402647	201636.525639	36.881344
1593.892470	202015.490536	36.886362
1595.476979	202390.607361	36.891380
1596.766844	202783.258319	36.896397
1598.603852	203156.432847	36.901415
1600.605498	203546.011922	36.906432
1601.752560	203924.256121	36.911450
1603.704502	204305.238805	36.916468
1605.081844	204701.935835	36.921485
1606.976868	205072.393165	36.926503
1608.628641	205470.864571	36.931520
1610.039563	205851.220636	36.936538
1612.064547	206225.039545	36.941556
1613.461521	206609.071173	36.946573
1615.134096	206986.392949	36.951591
1617.020790	207370.258500	36.956608
1618.784400	207739.036039	36.961626
1620.584818	208121.598893	36.966644
1621.885760	208498.214634	36.971661
1623.647642	208877.105063	36.976679
1625.501475	209263.892829	36.981696
1626.624312	209646.041434	36.986714
1628.243813	210012.338832	36.991732
1629.894395	210411.139700	36.996749
1631.362848	210790.417442	37.001767
1633.274041	211167.439644	37.006784
1634.434528	211558.149210	37.011802
1636.321818	211940.232622	37.016820
1637.459492	212336.054149	37.021837
1638.991224	212710.860009	37.026855
1640.885095	213090.458429	37.031872
1642.451419	213465.591900	37.036890
1644.156474	213825.821311	37.041908
1645.337339	214213.847076	37.046925
1647.157192	214582.670149	37.051943
1648.238196	214965.737695	37.056960
1650.116418	215351.468839	37.061978
1651.864138	215738.543793	37.066996
1653.086381	216128.399279	37.072013
1655.067325	216514.016569	37.077031
1656.597222	216908.294395	37.082048
1658.178784	217305.663832	37.087066
1659.496837	217704.272104	37.092084
1661.138256	218117.432529	37.097101
1662.764380	218514.545428	37.102119
1664.771282	218931.331551	37.107136
1666.189009	219335.441225	37.112154
1668.260989	219743.787559	37.117172
1669.565390	220170.269970	37.122189
1671.082165	220577.288906	37.127207
1673.349471	220992.186066	37.132224
1674.415515	221408.502396	37.137242
1676.439748	221822.884084	37.142260
1678.468639	222245.546692	37.147277
1679.905483	222671.255005	37.152295
1681.810864	223088.404116	37.157312
1683.755065	223511.847401	37.162330
1685.615008	223950.545895	37.167348
1687.076402	224419.867673	37.172365
1688.822565	224832.020148	37.177383
1690.530791	225261.198200	37.182400
1692.230891	225670.236937	37.187418
1694.139429	226101.467620	37.192436
1695.828324	226526.462232	37.197453
1697.287459	226941.590135	37.202471
1699.367172	227370.917224	37.207488
1700.615650	227788.902059	37.212506
1703.024768	228218.380701	37.217524
1704.832743	228651.592287	37.222541
1706.305238	229065.276794	37.227559
1708.039094	229484.532916	37.232576
1709.943557	229911.128329	37.237594
1711.449371	230338.806900	37.242612
1713.313555	230765.132094	37.247629
1715.174700	231176.320043	37.252647
1717.142443	231606.847119	37.257664
1718.715416	232037.288218	37.262682
1720.221552	232455.523587	37.267700
1722.172804	232887.377830	37.272717
1723.423399	233303.574752	37.277735
1725.530848	233740.130140	37.282752
1727.334946	234159.362193	37.287770
1728.892730	234581.633360	37.292788
1730.931666	235013.808924	37.297805
1732.590896	235440.104296	37.302823
1734.246724	235868.382593	37.307840
1735.812113	236299.598049	37.312858
1737.660623	236733.409546	37.317876
1739.475775	237164.738173	37.322893
1741.212361	237591.432197	37.327911
1743.123845	238019.927212	37.332928
1744.837951	238456.940036	37.337946
1746.891290	238866.615910	37.342964
1748.297320	239298.702599	37.347981
1750.011866	239719.714654	37.352999
1751.766973	240148.747940	37.358016
1753.175332	240575.832544	37.363034
1754.998865	241004.424325	37.368052
1756.788446	241414.504157	37.373069
1758.457113	241824.401447	37.378087
1760.284991	242229.853097	37.383104
1761.620486	242649.027883	37.388122
1763.591874	243060.502960	37.393140
1765.055150	243485.627591	37.398157
1766.681474	243898.380276	37.403175
1768.391386	244317.978489	37.408192
1769.977054	244747.098452	37.413210
1771.703062	245176.805525	37.418228
1773.469692	245605.566590	37.423245
1775.090002	246052.388408	37.428263
1777.116968	246485.527743	37.433280
1778.437174	246923.229866	37.438298
1780.460921	247369.783569	37.443316
1782.181276	247817.505655	37.448333
1784.282465	248260.415014	37.453351
1785.907678	248700.024880	37.458368
1787.595080	249165.942483	37.463386
1789.498843	249618.793081	37.468404
1791.162846	250071.505905	37.473421
1793.291897	250528.486281	37.478439
1795.495135	250984.108449	37.483456
1796.677560	251438.578632	37.488474
1798.641600	251893.758391	37.493492
1800.231223	252361.397080	37.498509
1802.027505	252824.403991	37.503527
1804.082526	253286.911212	37.508544
1806.055331	253765.690359	37.513562
1807.845657	254239.368456	37.518580
1809.372892	254699.804335	37.523597
1811.382192	255178.222525	37.528615
1813.235011	255639.671954	37.533632
1814.884860	256108.953865	37.538650
1816.978048	256581.439715	37.543668
1819.137240	257059.097046	37.548685
1821.026415	257530.600648	37.553703
1822.720383	258000.256701	37.558720
1824.546802	258478.680453	37.563738
1826.406814	258954.939381	37.568756
1828.769627	259420.395056	37.573773
1830.523104	259880.819849	37.578791
1832.837565	260353.726561	37.583808
1834.226947	260822.137147	37.588826
1836.424423	261283.352044	37.593844
1838.258648	261753.975194	37.598861
1840.065491	262217.947038	37.603879
1842.197098	262676.860615	37.608896
1844.053778	263151.112133	37.613914
1845.790723	263601.123091	37.618932
1847.529004	264069.220665	37.623949
1849.185807	264532.352373	37.628967
1851.579190	265000.569778	37.633984
1853.235890	265469.899218	37.639002
1855.243403	265925.986123	37.644020
1857.158332	266404.137847	37.649037
1858.522956	266863.480110	37.654055
1860.894833	267327.304366	37.659072
1862.898372	267784.177750	37.664090
1864.473889	268254.508734	37.669108
1866.545741	268713.275079	37.674125
1868.500043	269179.147737	37.679143
1870.679407	269630.350581	37.684160
1872.172475	270089.490298	37.689178
1874.051942	270552.655471	37.694196
1875.992797	271010.551492	37.699213
1877.929684	271461.436360	37.704231
1879.654086	271918.401530	37.709248
1881.252880	272361.466072	37.714266
1883.097132	272796.233549	37.719284
1884.913445	273234.332725	37.724301
1886.813937	273671.833051	37.729319
1888.545447	274121.909435	37.734336
1890.136231	274570.331721	37.739354
1892.441382	275010.354049	37.744372
1894.102173	275469.203584	37.749389
1895.251561	275922.649785	37.754407
1897.756252	276377.497057	37.759424
1899.363636	276836.301939	37.764442
1901.226381	277300.804612	37.769460
1902.846419	277763.085581	37.774477
1904.314717	278237.558209	37.779495
1906.560252	278720.665112	37.784512
1908.134130	279202.891096	37.789530
1909.912087	279687.749406	37.794548
1911.963481	280170.630807	37.799565
1913.935775	280665.031046	37.804583
1915.551719	281161.901967	37.809600
1917.823909	281666.690079	37.814618
1919.290051	282174.531029	37.819636
1921.464336	282677.986104	37.824653
1923.595299	283181.142019	37.829671
1925.418934	283689.833844	37.834688
1927.314995	284199.350360	37.839706
1929.133575	284703.111973	37.844724
1931.488349	285214.530757	37.849741
1933.208285	285728.668964	37.854759
1935.157074	286231.515015	37.859776
1937.209572	286744.959778	37.864794
1939.046431	287271.291104	37.869812
1941.241242	287792.405045	37.874829
1943.170180	288310.817684	37.879847
1945.428817	288819.597953	37.884864
1947.362836	289337.421632	37.889882
1949.139805	289855.218421	37.894900
1951.287534	290370.411921	37.899917
1953.069920	290892.750294	37.904935
1955.489086	291417.318157	37.909952
1957.678947	291933.819120	37.914970
1959.505038	292452.841741	37.919988
1962.102597	292965.943630	37.925005
1964.028680	293491.549133	37.930023
1965.938527	293988.580631	37.935040
1967.981172	294515.229027	37.940058
1969.819199	295024.205547	37.945076
1971.910746	295527.245313	37.950093
1973.794806	296049.391648	37.955111
1975.946509	296553.737518	37.960128
1977.915180	297077.617438	37.965146
1979.929843	297590.362604	37.970164
1981.843436	298094.080098	37.975181
1984.256287	298612.342134	37.980199
1986.086806	299122.900440	37.985216
1988.374196	299630.409150	37.990234
1990.316695	300145.870969	37.995252
1992.478740	300643.972536	38.000269
1994.536067	301151.638358	38.005287
1996.760974	301660.645289	38.010304
1998.553654	302171.727242	38.015322
2000.051583	302665.026199	38.020340
2002.337607	303170.510010	38.025357
2004.107907	303682.603200	38.030375
2006.041540	304193.193508	38.035392
2008.105201	304704.241971	38.040410
2010.149713	305215.696988	38.045428
2012.307469	305712.451206	38.050445
2013.905217	306205.688766	38.055463
2015.953307	306691.027134	38.060480
2017.936992	307172.690945	38.065498
2019.715456	307662.715701	38.070516
2021.585189	308138.881865	38.075533
2023.687925	308636.364431	38.080551
2025.442462	309130.142936	38.085568
2027.622270	309627.505117	38.090586
2029.304597	310132.285502	38.095604
2031.579845	310629.473289	38.100621
2033.163164	311145.488060	38.105639
2034.960958	311648.182648	38.110656
2037.253767	312170.650621	38.115674
2039.064539	312689.690193	38.120692
2041.173481	313216.599899	38.125709
2043.150442	313745.330638	38.130727
2045.292651	314273.116144	38.135744
2047.566239	314807.605427	38.140762
2049.711236	315344.752902	38.145780
2051.551395	315863.358948	38.150797
2053.504931	316411.499839	38.155815
2055.747719	316949.583992	38.160832
2057.831641	317478.295002	38.165850
2059.696678	318034.868085	38.170868
2061.799789	318572.302489	38.175885
2063.861508	319125.507849	38.180903
2065.832855	319671.156863	38.185920
2068.227176	320229.935159	38.190938
2070.307911	320778.781738	38.195956
2072.581394	321325.839921	38.200973
2074.563650	321883.250259	38.205991
2076.552600	322437.912483	38.211008
2078.989737	322991.531066	38.216026
2081.219286	323542.868572	38.221044
2083.227568	324093.501457	38.226061
2085.242000	324655.452273	38.231079
2086.992347	325211.703545	38.236096
2089.473156	325762.015033	38.241114
2091.585483	326340.284901	38.246132
2093.848448	326896.055276	38.251149
2095.918659	327461.195282	38.256167
2097.712100	328020.688605	38.261184
2100.236060	328585.539822	38.266202
2102.332027	329156.625453	38.271220
2104.542761	329709.178963	38.276237
2106.959723	330264.384159	38.281255
2108.977050	330832.013408	38.286272
2111.030040	331389.349404	38.291290
2113.109907	331958.911736	38.296308
2115.435077	332513.932162	38.301325
2117.825327	333079.039902	38.306343
2119.737935	333640.158931	38.311360
2121.944196	334200.639822	38.316378
2123.964940	334758.987765	38.321396
2126.364363	335313.408855	38.326413
2128.467483	335885.896218	38.331431
2130.669882	336445.897220	38.336448
2132.863337	337001.730706	38.341466
2134.947419	337562.018485	38.346484
2137.252601	338123.075959	38.351501
2139.092085	338676.335330	38.356519
2141.578036	339232.934070	38.361536
2143.580018	339794.378532	38.366554
2145.116341	340356.731205	38.371572
2147.612900	340917.294565	38.376589
2149.523839	341481.501715	38.381607
2151.872782	342048.041343	38.386624
2153.949804	342599.187433	38.391642
2155.911537	343149.990957	38.396660
2158.160621	343677.974207	38.401677
2160.106298	344221.204630	38.406695
2162.319728	344760.247683	38.411712
2164.481224	345297.643470	38.416730
2166.161227	345844.096973	38.421748
2168.353154	346392.921374	38.426765
2170.181692	346948.626221	38.431783
2172.310386	347496.965760	38.436800
2174.280662	348047.913485	38.441818
2176.145039	348616.179878	38.446836
2178.300221	349191.268507	38.451853
2180.252797	349779.833261	38.456871
2182.461080	350358.679383	38.461888
2184.632300	350953.333794	38.466906
2186.624569	351543.391219	38.471924
2188.869091	352139.565448	38.476941
2191.213943	352745.636858	38.481959
2193.240959	353328.609909	38.486976
2195.584111	353944.967143	38.491994
2197.632698	354544.083974	38.497012
2199.737024	355155.286682	38.502029
2201.870974	355766.018914	38.507047
2204.181530	356392.876040	38.512064
2206.254313	357008.548043	38.517082
2208.523578	357640.620012	38.522100
2210.940788	358258.956759	38.527117
2213.181704	358899.995807	38.532135
2215.566010	359515.375759	38.537152
2217.968152	360142.667849	38.542170
2219.908215	360781.620850	38.547188
2222.121664	361405.905134	38.552205
2224.707193	362040.824303	38.557223
2226.871523	362676.766792	38.562240
2229.126529	363316.337137	38.567258
2231.240250	363957.214085	38.572276
2233.503522	364600.617921	38.577293
2236.157590	365241.942412	38.582311
2238.406764	365880.075918	38.587328
2240.965502	366518.299800	38.592346
2243.056140	367158.543369	38.597364
2245.314540	367800.574683	38.602381
2247.717846	368436.838362	38.607399
2249.849630	369082.318169	38.612416
2252.566669	369710.112221	38.617434
2254.655620	370358.924825	38.622452
2257.081633	370999.756680	38.627469
2259.734358	371630.216819	38.632487
2261.531898	372267.122466	38.637504
2264.167716	372900.936365	38.642522
2266.451689	373544.206412	38.647540
2268.983214	374169.797522	38.652557
2271.305175	374809.233987	38.657575
2273.503071	375441.781112	38.662592
2276.098445	376071.081103	38.667610
2278.284036	376710.099398	38.672628
2280.515081	377342.479533	38.677645
2282.902217	377961.001610	38.682663
2284.820198	378593.866711	38.687680
2287.437097	379223.054529	38.692698
2289.491628	379863.151077	38.697716
2291.631155	380496.045342	38.702733
2294.528782	381124.999002	38.707751
2296.384865	381765.624290	38.712768
2298.980093	382391.104659	38.717786
2301.139039	383019.789152	38.722804
2303.311645	383643.033408	38.727821
2305.613342	384274.839463	38.732839
2307.499317	384883.756747	38.737856
2310.118635	385479.763492	38.742874
2312.057309	386095.215582	38.747892
2314.303508	386705.154319	38.752909
2316.609285	387304.373075	38.757927
2318.655918	387917.895973	38.762944
2320.896508	388541.591228	38.767962
2323.039533	389164.200090	38.772980
2325.256400	389784.401439	38.777997
2327.803592	390412.875746	38.783015
2329.958027	391058.233573	38.788032
2332.041048	391691.904120	38.793050
2334.510357	392343.621306	38.798068
2336.679667	392983.993191	38.803085
2338.902119	393635.621944	38.808103
2341.035789	394295.970248	38.813120
2343.364893	394940.684313	38.818138
2345.682961	395609.134374	38.823156
2347.705285	396279.493647	38.828173
2350.026393	396951.461067	38.833191
2352.136427	397630.341265	38.838208
2354.461153	398309.803823	38.843226
2356.856515	399011.083568	38.848244
2358.922891	399709.765107	38.853261
2361.875875	400400.858561	38.858279
2363.723381	401102.203104	38.863296
2366.347637	401800.488175	38.868314
2368.380305	402502.578476	38.873332
2370.726438	403221.145403	38.878349
2373.715759	403930.212920	38.883367
2376.149244	404649.083516	38.888384
2378.685705	405368.298570	38.893402
2381.157498	406079.423554	38.898420
2383.259710	406794.290045	38.903437
2385.777972	407510.538610	38.908455
2388.309861	408233.074161	38.913472
2390.820359	408953.947355	38.918490
2393.277687	409677.292625	38.923508
2395.828489	410400.349675	38.928525
2398.483399	411118.987753	38.933543
2400.467779	411852.763167	38.938560
2403.363938	412563.166023	38.943578
2405.863830	413284.025233	38.948596
2408.391442	414011.344038	38.953613
2411.072270	414725.067158	38.958631
2413.026072	415447.527027	38.963648
2415.567333	416171.364010	38.968666
2418.167468	416893.626082	38.973684
2420.416854	417621.724982	38.978701
2423.505439	418338.522151	38.983719
2425.737406	419068.709714	38.988736
2428.461177	419772.105270	38.993754
2431.002620	420495.616626	38.998772
2433.266432	421205.910052	39.003789
2435.792235	421915.380408	39.008807
2438.203139	422634.394879	39.013824
2440.569278	423359.953363	39.018842
2443.212273	424080.482443	39.023860
2445.427817	424793.161879	39.028877
2447.969993	425506.981784	39.033895
2450.715287	426239.784618	39.038912
2453.339407	426947.928447	39.043930
2455.872250	427658.142266	39.048948
2458.114625	428375.977006	39.053965
2460.366604	429076.727796	39.058983
2462.880508	429799.486741	39.064000
2465.152129	430504.596370	39.069018
2468.083515	431217.422276	39.074036
2470.166700	431900.247950	39.079053
2472.496669	432580.279589	39.084071
2474.877016	433266.610100	39.089088
2477.537519	433950.444551	39.094106
2479.600299	434638.507669	39.099124
2482.110820	435323.540839	39.104141
2484.470188	436015.360252	39.109159
2486.421800	436711.730153	39.114176
2488.677094	437424.374759	39.119194
2491.367604	438131.156077	39.124212
2493.422379	438852.239863	39.129229
2496.012604	439563.597690	39.134247
2497.960863	440297.859761	39.139264
2500.603740	441042.760627	39.144282
2503.126619	441770.706145	39.149300
2505.177272	442514.997405	39.154317
2507.571599	443261.179948	39.159335
2510.061716	444027.305202	39.164352
2512.605169	444792.686484	39.169370
2515.194478	445558.134409	39.174388
2517.685482	446335.762895	39.179405
2520.237856	447089.628808	39.184423
2522.420834	447878.381018	39.189440
2525.144074	448650.272551	39.194458
2527.797424	449436.309865	39.199476
2529.989011	450234.886860	39.204493
2532.948637	451015.200820	39.209511
2535.411749	451818.427058	39.214528
2538.014672	452613.963042	39.219546
2540.777545	453413.740695	39.224564
2543.185422	454214.709137	39.229581
2546.084546	455008.081711	39.234599
2548.909326	455822.672832	39.239616
2551.354650	456618.636782	39.244634
2553.893759	457428.559330	39.249652
2556.568029	458235.596041	39.254669
2559.031495	459031.664685	39.259687
2561.840632	459850.444691	39.264704
2564.686829	460651.390900	39.269722
2567.307121	461452.089522	39.274740
2569.690075	462271.143949	39.279757
2572.659309	463069.141872	39.284775
2575.039443	463888.079267	39.289792
2577.644009	464692.339011	39.294810
2580.967301	465495.739600	39.299828
2583.104505	466307.439282	39.304845
2585.823647	467122.546523	39.309863
2588.941002	467931.085485	39.314880
2591.657595	468739.050258	39.319898
2594.609565	469541.080836	39.324916
2596.731346	470332.907248	39.329933
2599.452774	471133.948902	39.334951
2601.989649	471935.846064	39.339968
2604.538921	472737.505078	39.344986
2607.521801	473533.147790	39.350004
2609.694243	474338.791601	39.355021
2612.615425	475138.316520	39.360039
2615.429940	475929.894336	39.365056
2617.674173	476747.039789	39.370074
2620.409626	477546.592520	39.375092
2623.034289	478350.421729	39.380109
2625.445493	479141.978684	39.385127
2627.929226	479953.841188	39.390144
2630.618465	480766.037563	39.395162
2633.367563	481562.331855	39.400180
2635.412339	482385.418551	39.405197
2637.974986	483188.690425	39.410215
2640.955138	483989.736882	39.415232
2643.385010	484786.243849	39.420250
2645.915197	485557.405655	39.425268
2648.306909	486342.338574	39.430285
2650.700894	487117.897357	39.435303
2653.322269	487917.563580	39.440320
2655.983067	488704.416438	39.445338
2658.462481	489491.112385	39.450356
2660.699715	490292.600886	39.455373
2663.284824	491105.855237	39.460391
2665.790690	491920.598428	39.465408
2668.280218	492735.204878	39.470426
2671.195612	493559.996665	39.475444
2673.487163	494394.287503	39.480461
2676.138537	495213.694299	39.485479
2679.055998	496058.144008	39.490496
2681.015961	496920.720846	39.495514
2684.185401	497767.263451	39.500532
2686.580935	498624.787552	39.505549
2689.417797	499485.675584	39.510567
2691.908882	500344.155022	39.515584
2694.647490	501218.387104	39.520602
2697.262698	502090.475058	39.525620
2699.941447	502970.777526	39.530637
2702.793472	503842.683173	39.535655
2705.605860	504732.904765	39.540672
2708.199152	505628.963250	39.545690
2711.232489	506514.865661	39.550708
2714.056557	507406.955746	39.555725
2716.750630	508303.958801	39.560743
2719.383877	509196.888689	39.565760
2722.238264	510091.950408	39.570778
2725.534504	510979.378155	39.575796
2728.122321	511885.624111	39.580813
2731.129460	512793.412337	39.585831
2733.927099	513686.617310	39.590848
2736.304576	514595.917479	39.595866
2739.220435	515489.201925	39.600884
2741.956336	516400.152227	39.605901
2744.600548	517299.777315	39.610919
2747.592621	518218.791898	39.615936
2750.203000	519124.765700	39.620954
2753.529959	520034.950950	39.625972
2756.501496	520947.105422	39.630989
2758.938052	521846.347688	39.636007
2762.055968	522763.154788	39.641024
2764.689965	523680.489918	39.646042
2767.758498	524579.868738	39.651060
2770.515067	525484.079940	39.656077
2773.249976	526391.513481	39.661095
2776.033668	527303.466194	39.666112
2778.687615	528208.033067	39.671130
2781.594016	529121.263884	39.676148
2784.610658	530039.505048	39.681165
2787.290504	530949.538680	39.686183
2790.524939	531861.287016	39.691200
2793.064312	532762.421846	39.696218
2795.686726	533670.835965	39.701236
2798.558834	534590.677726	39.706253
2801.424050	535505.479835	39.711271
2804.276431	536419.219599	39.716288
2807.299468	537331.464194	39.721306
2809.922896	538241.854886	39.726324
2812.697046	539161.319875	39.731341
2815.606210	540070.188242	39.736359
2818.173097	540978.400832	39.741376
2820.893002	541894.327042	39.746394
2823.757283	542812.735271	39.751412
2826.610107	543706.087291	39.756429
2829.024254	544596.336370	39.761447
2832.178437	545475.091020	39.766464
2834.987144	546352.640192	39.771482
2837.921784	547227.699358	39.776500
2840.574172	548117.532556	39.781517
2843.285445	548982.812820	39.786535
2846.189030	549869.172862	39.791552
2849.039778	550762.170428	39.796570
2851.770662	551640.350234	39.801588
2854.394531	552529.348386	39.806605
2857.179660	553435.049295	39.811623
2860.156743	554327.188437	39.816640
2862.875508	555236.247254	39.821658
2865.404897	556143.114914	39.826676
2868.390983	557065.221961	39.831693
2871.056445	557991.840223	39.836711
2873.973610	558901.219959	39.841728
2876.623248	559849.063976	39.846746
2879.740727	560767.727198	39.851764
2882.447790	561719.797744	39.856781
2885.452926	562660.850722	39.861799
2888.582890	563611.709529	39.866816
2891.135453	564555.965145	39.871834
2894.495559	565497.257098	39.876852
2897.297425	566456.297854	39.881869
2900.474053	567404.561253	39.886887
2903.434241	568357.509789	39.891904
2906.475699	569324.430610	39.896922
2909.482532	570281.093859	39.901940
2912.287592	571239.023623	39.906957
2914.996668	572203.020207	39.911975
2918.179145	573172.436052	39.916992
2920.742734	574143.886792	39.922010
2923.627778	575112.499877	39.927028
2926.801003	576090.724545	39.932045
2929.677714	577082.066304	39.937063
2932.948885	578055.956579	39.942080
2935.528129	579054.464380	39.947098
2938.362802	580037.049492	39.952116
2941.567707	581029.827201	39.957133
2944.735085	582030.705514	39.962151
2947.572730	583007.786933	39.967168
2950.282635	584017.103141	39.972186
2953.356388	585014.493171	39.977204
2956.492369	586007.830368	39.982221
2959.426484	587020.519676	39.987239
2962.590544	588021.707433	39.992256
2965.273535	589016.575765	39.997274
2968.366859	590020.565605	40.002292
2971.453011	591029.684019	40.007309
2974.339819	592043.259579	40.012327
2977.480462	593040.673153	40.017344
2980.606590	594051.582283	40.022362
2983.593069	595058.019281	40.027380
2986.857151	596056.810513	40.032397
2989.747194	597071.355904	40.037415
2993.326316	598064.063506	40.042432
2996.019029	599067.249056	40.047450
2998.962543	600074.012078	40.052468
3002.239285	601067.664295	40.057485
3005.092043	602079.274536	40.062503
3008.149510	603064.429536	40.067520
3011.214747	604075.928897	40.072538
3014.323907	605072.966261	40.077556
3017.326035	606071.135157	40.082573
3020.250028	607080.088778	40.087591
3023.426490	608069.045069	40.092608
3026.446035	609047.633265	40.097626
3029.652777	610015.949171	40.102644
3032.532742	610967.576423	40.107661
3035.434560	611917.218252	40.112679
3038.166402	612867.307432	40.117696
3040.783045	613819.485047	40.122714
3044.187531	614783.753421	40.127732
3047.208967	615738.249792	40.132749
3050.043696	616710.894679	40.137767
3053.211158	617677.499061	40.142784
3056.159585	618645.754041	40.147802
3058.767124	619628.675824	40.152820
3061.861716	620606.880197	40.157837
3064.636035	621593.045886	40.162855
3067.870314	622587.141783	40.167872
3070.454829	623598.642657	40.172890
3073.463858	624604.032765	40.177908
3076.707438	625617.833229	40.182925
3079.322098	626641.782273	40.187943
3082.276896	627665.127475	40.192960
3085.605462	628700.649206	40.197978
3088.476647	629738.592354	40.202996
3091.676805	630786.066954	40.208013
3094.498630	631839.841074	40.213031
3097.683299	632892.800733	40.218048
3100.568092	633963.675464	40.223066
3103.672440	635025.918631	40.228084
3107.072723	636097.587486	40.233101
3109.862029	637187.162412	40.238119
3113.076743	638259.686388	40.243136
3115.885967	639345.288061	40.248154
3119.064143	640443.486061	40.253172
3122.565847	641531.785763	40.258189
3125.548750	642634.470089	40.263207
3129.096793	643727.914913	40.268224
3131.839474	644835.537309	40.273242
3135.156286	645948.927460	40.278260
3138.601867	647040.635437	40.283277
3141.697743	648164.536577	40.288295
3144.925877	649277.722742	40.293312
3148.136174	650390.090223	40.298330
3151.163626	651506.151224	40.303348
3154.607124	652607.817064	40.308365
3157.740996	653738.458649	40.313383
3160.614318	654856.210636	40.318400
3164.025350	655980.770696	40.323418
3167.220408	657107.827513	40.328436
3170.361945	658222.761428	40.333453
3174.044716	659347.686759	40.338471
3176.876109	660471.626573	40.343488
3180.352476	661608.074433	40.348506
3183.548456	662728.804780	40.353524
3186.895513	663852.963521	40.358541
3189.809747	664982.237789	40.363559
3193.216929	666104.331315	40.368576
3196.320425	667237.836336	40.373594
3199.716324	668360.362875	40.378612
3203.138459	669487.179466	40.383629
3206.125479	670625.124365	40.388647
3209.453581	671762.925588	40.393664
3213.028911	672881.802337	40.398682
3216.065740	673994.717874	40.403700
3219.682177	675104.273567	40.408717
3222.524696	676239.224959	40.413735
3225.932957	677350.535566	40.418752
3229.095505	678475.767374	40.423770
3232.280278	679598.672247	40.428788
3235.903473	680711.332158	40.433805
3238.713658	681830.747356	40.438823
3241.836002	682912.274351	40.443840
3245.333603	683991.773876	40.448858
3248.430560	685056.363476	40.453876
3251.592740	686123.101635	40.458893
3254.430821	687203.370987	40.463911
3257.814695	688279.648494	40.468928
3260.808993	689365.838354	40.473946
3263.822180	690451.496763	40.478964
3266.868864	691551.260001	40.483981
3269.609371	692647.762837	40.488999
3272.966376	693760.450385	40.494016
3276.103275	694881.021209	40.499034
3279.394345	696013.477295	40.504052
3282.248204	697138.123896	40.509069
3284.975440	698283.870439	40.514087
3288.497261	699437.715443	40.519104
3292.000790	700597.607978	40.524122
3294.734450	701760.298557	40.529140
3298.182365	702927.572966	40.534157
3301.457249	704110.773927	40.539175
3304.532442	705298.206056	40.544192
3308.024511	706495.957849	40.549210
3310.959697	707691.356185	40.554228
3314.310624	708879.932595	40.559245
3317.431626	710090.862899	40.564263
3320.855301	711319.197228	40.569280
3324.229042	712539.342680	40.574298
3327.499843	713771.060107	40.579316
3331.048917	714996.316455	40.584333
3334.455685	716242.992202	40.589351
3337.703601	717470.708656	40.594368
3341.405183	718718.254098	40.599386
3344.618158	719961.736778	40.604404
3348.281158	721209.756383	40.609421
3351.375038	722451.303589	40.614439
3355.048983	723698.649682	40.619456
3358.400498	724960.639831	40.624474
3361.417588	726228.718593	40.629492
3365.172510	727476.219461	40.634509
3368.800576	728734.074516	40.639527
3372.293100	729994.919241	40.644544
3375.638427	731261.420721	40.649562
3378.718817	732521.150257	40.654580
3382.572502	733782.234584	40.659597
3385.892820	735056.094417	40.664615
3389.471889	736316.431271	40.669632
3393.033142	737574.598345	40.674650
3396.238338	738843.530921	40.679668
3399.826004	740109.829774	40.684685
3403.438707	741385.886783	40.689703
3406.802868	742643.628361	40.694720
3410.262675	743911.607941	40.699738
3413.357348	745196.552118	40.704756
3417.063655	746448.598990	40.709773
3420.520521	747737.404221	40.714791
3423.953318	748995.396255	40.719808
3427.287139	750268.968293	40.724826
3430.799491	751548.705866	40.729844
3434.484047	752812.292747	40.734861
3437.626516	754085.315770	40.739879
3440.964363	755349.084271	40.744896
3444.374891	756617.850691	40.749914
3447.780627	757903.783117	40.754932
3451.150935	759175.772590	40.759949
3454.831959	760465.113927	40.764967
3457.625018	761746.411332	40.769984
3461.849490	763025.779367	40.775002
3465.149119	764299.592717	40.780007
3468.827108	765516.959274	40.785012
3471.800121	766673.761392	40.790016
3475.150532	767764.821283	40.795021
3478.608650	768803.221465	40.800026
3481.273243	769776.961870	40.805031
3484.223506	770666.823817	40.810036
3486.939311	771504.991935	40.815040
3489.510005	772274.327958	40.820045
3492.531521	772975.149126	40.825050
3494.693376	773617.293934	40.830055
3496.868596	774182.069316	40.835060
3499.384903	774697.259445	40.840064
3501.158714	775146.706782	40.845069
3503.324799	775550.028452	40.850074
3505.005189	775895.413499	40.855079
3506.892343	776185.315980	40.860084
3508.188668	776438.678930	40.865088
3509.919127	776633.136207	40.870093
3511.226983	776779.220252	40.875098
3512.828613	776903.298825	40.880103
3513.984655	776969.709006	40.885108
3515.342103	776996.263321	40.890112
3516.135008	777012.721224	40.895117
3517.516675	776954.901540	40.900122
3518.051464	776900.469757	40.905127
3518.861785	776797.111614	40.910132
3519.717600	776658.154032	40.915136
3519.867097	776525.562027	40.920141
3520.907597	776358.361112	40.925146
3521.620189	776179.936861	40.930151
3522.151257	775970.079700	40.935156
3522.775757	775749.025381	40.940160
3522.960771	775510.017177	40.945165
3523.333422	775244.826103	40.950170
3523.640149	774969.739526	40.955175
3524.083100	774697.032903	40.960180
3524.304788	774395.595623	40.965184
3524.538359	774090.204508	40.970189
3525.042784	773753.435803	40.975194
3525.072863	773436.822977	40.980199
3525.606245	773088.199490	40.985204
3525.415466	772743.224973	40.990208
3525.623142	772390.484861	40.995213
3526.131324	772028.417966	41.000218
3525.792080	771674.452983	41.005223
3525.949123	771291.915706	41.010228
3525.905846	770923.087211	41.015232
3525.391429	770561.067521	41.020237
3526.065424	770172.228690	41.025242
3525.759223	769785.846729	41.030247
3525.760649	769398.950444	41.035252
3525.755000	769019.180353	41.040256
3525.635500	768626.005428	41.045261
3525.981822	768221.003661	41.050266
3525.947273	767837.974538	41.055271
3525.977040	767431.010489	41.060276
3525.854515	767034.252436	41.065280
3525.802159	766634.750569	41.070285
3526.089770	766227.875502	41.075290
3525.474124	765837.592786	41.080295
3525.571124	765424.493751	41.085300
3525.456525	765021.612662	41.090304
3525.246462	764620.599264	41.095309
3525.282977	764224.651917	41.100314
3524.892828	763828.260847	41.105319
3524.840566	763431.891795	41.110324
3524.947351	763036.314013	41.115328
3524.826998	762627.781815	41.120333
3524.974583	762229.195701	41.125338
3524.185313	761828.868516	41.130343
3524.125588	761432.050092	41.135348
3524.282311	761047.063655	41.140352
3523.898284	760651.540220	41.145357
3524.033083	760248.806354	41.150362
3523.788648	759874.729371	41.155367
3523.648233	759477.328265	41.160372
3523.251455	759108.320573	41.165376
3523.089750	758722.923009	41.170381
3523.156609	758339.491475	41.175386
3523.126281	757962.176013	41.180391
3522.714855	757584.657866	41.185396
3522.755148	757206.849151	41.190400
3522.643647	756828.701215	41.195405
3522.638231	756456.440222	41.200410
3522.413738	756093.329162	41.205415
3522.451440	755715.200209	41.210420
3522.165244	755344.955269	41.215424
3521.902552	754977.650699	41.220429
3521.965384	754610.126765	41.225434
3521.627510	754251.538551	41.230439
3521.330820	753894.259949	41.235444
3521.214435	753532.342808	41.240448
3521.026328	753189.580205	41.245453
3520.992564	752830.875563	41.250458
3520.790179	752495.047385	41.255463
3520.866196	752128.785398	41.260468
3520.531718	751786.626503	41.265472
3520.097983	751449.803118	41.270477
3520.228417	751106.944793	41.275482
3520.075670	750775.627249	41.280487
3519.940575	750433.573157	41.285492
3519.576676	750092.875466	41.290496
3519.193648	749766.789142	41.295501
3519.673172	749445.487455	41.300506
3519.374543	749113.381782	41.305511
3519.148565	748787.179003	41.310516
3519.383380	748470.422919	41.315520
3519.195483	748143.692755	41.320525
3518.996709	747816.456515	41.325530
3518.662548	747494.417631	41.330535
3517.864103	747174.764634	41.335540
3518.132113	746866.190832	41.340544
3517.681437	746561.924206	41.345549
3518.171818	746259.121696	41.350554
3518.043235	745958.831362	41.355559
3517.659835	745657.830054	41.360564
3517.274470	745349.353464	41.365568
3517.176860	745057.673817	41.370573
3517.056251	744765.888238	41.375578
3516.992778	744487.825640	41.380583
3516.829440	744194.789963	41.385588
3516.642573	743909.311515	41.390592
3516.440558	743628.818787	41.395597
3516.758445	743339.083385	41.400602
3516.303020	743067.512194	41.405607
3516.384095	742787.684523	41.410612
3516.161927	742503.100372	41.415616
3515.994274	742224.777162	41.420621
3516.124832	741952.625957	41.425626
3515.959235	741680.662533	41.430631
3515.734789	741408.353256	41.435636
3515.813413	741139.100463	41.440640
3515.558795	740884.088077	41.445645
3515.411455	740613.865473	41.450650
3515.080792	740363.003505	41.455655
3515.419293	740085.807631	41.460660
3515.201516	739823.978527	41.465664
3514.755134	739581.520004	41.470669
3514.582327	739321.793999	41.475674
3514.085009	739076.805567	41.480679
3514.067157	738825.348757	41.485684
3513.707541	738583.735978	41.490688
3513.482096	738355.748717	41.495693
3513.686818	738119.866861	41.500698
3513.466022	737894.636289	41.505703
3513.637023	737657.905207	41.510708
3513.819500	737433.188905	41.515712
3513.157426	737206.230315	41.520717
3513.630907	736971.804167	41.525722
3513.637038	736739.872890	41.530727
3513.287135	736517.197921	41.535732
3513.209089	736284.426044	41.540736
3513.043557	736068.240520	41.545741
3513.197077	735834.477125	41.550746
3512.781879	735623.517189	41.555751
3512.621098	735403.403122	41.560756
3512.745416	735177.296746	41.565760
3512.256946	734977.072092	41.570765
3512.486706	734750.292876	41.575770
3512.372927	734547.817924	41.580775
3512.114574	734329.521916	41.585780
3512.118913	734126.769400	41.590784
3511.737779	733929.867001	41.595789
3511.669937	733721.819480	41.600794
3511.782816	733527.746530	41.605799
3511.479480	733332.202815	41.610804
3511.262033	733128.372583	41.615808
3511.175098	732935.209411	41.620813
3511.686040	732743.972977	41.625818
3511.535094	732566.456385	41.630823
3511.270956	732364.446426	41.635828
3511.481396	732166.611307	41.640832
3510.646962	731981.321958	41.645837
3510.576305	731803.676349	41.650842
3510.554007	731609.926176	41.655847
3510.590035	731435.275379	41.660852
3510.615869	731252.551030	41.665856
3510.273914	731077.311056	41.670861
3510.215158	730895.682021	41.675866
3510.183042	730736.081570	41.680871
3510.071923	730552.125962	41.685876
3510.152993	730388.934412	41.690880
3510.226835	730219.054965	41.695885
3510.134713	730048.456426	41.700890
3509.863093	729879.022993	41.705895
3510.081675	729707.722261	41.710900
3509.825611	729539.220206	41.715904
3509.802657	729374.886274	41.720909
3509.828596	729199.842334	41.725914
3509.551483	729040.694727	41.730919
3509.280661	728876.589702	41.735924
3509.410925	728717.913524	41.740928
3509.039715	728566.103127	41.745933
3509.003883	728415.076745	41.750938
3509.022901	728267.506079	41.755943
3509.164522	728109.262016	41.760948
3508.973446	727945.521410	41.765952
3508.735866	727813.044455	41.770957
3508.931775	727664.987900	41.775962
3509.029932	727510.207197	41.780967
3508.709747	727362.428362	41.785972
3508.767159	727213.197440	41.790976
3508.677504	727063.690767	41.795981
3508.523412	726927.866279	41.800986
3508.239041	726779.724202	41.805991
3508.067076	726635.375988	41.810996
3508.370245	726494.662980	41.816000
3508.252418	726374.777509	41.821005
3508.428884	726229.720617	41.826010
3507.997398	726103.590167	41.831015
3508.110065	725958.836293	41.836020
3508.087572	725827.778273	41.841024
3508.043441	725705.987938	41.846029
3507.955249	725565.373029	41.851034
3507.991451	725437.173162	41.856039
3507.666695	725306.453945	41.861044
3507.805754	725177.241989	41.866048
3507.737888	725045.683414	41.871053
3507.529822	724913.898052	41.876058
3507.527065	724792.136912	41.881063
3507.751345	724668.056887	41.886068
3507.424070	724550.954557	41.891072
3507.480299	724433.242216	41.896077
3507.304484	724296.039649	41.901082
3507.428489	724178.857670	41.906087
3507.179555	724058.365269	41.911092
3507.296861	723939.248076	41.916096
3506.796079	723824.047375	41.921101
3507.103059	723697.807895	41.926106
3506.964242	723598.950077	41.931111
3506.971917	723486.535629	41.936116
3507.347760	723365.384942	41.941120
3506.769608	723255.046507	41.946125
3506.930001	723138.587258	41.951130
3506.734951	723041.962566	41.956135
3506.757876	722915.262251	41.961140
3506.530774	722806.446177	41.966144
3506.645290	722703.966909	41.971149
3506.585483	722583.719238	41.976154
3506.512736	722479.483501	41.981159
3506.498647	722383.713582	41.986164
3506.593578	722288.370743	41.991168
3506.415510	722179.736634	41.996173
3506.466765	722061.396426	42.001178
3506.047940	721966.729421	42.006183
3506.365731	721863.958391	42.011188
3506.391325	721750.525894	42.016192
3506.082158	721654.994471	42.021197
3506.537653	721546.098934	42.026202
3506.019582	721456.449715	42.031207
3505.792825	721351.035295	42.036212
3506.189517	721261.332399	42.041216
3505.811115	721179.242691	42.046221
3505.996678	721082.135779	42.051226
3505.998780	720983.719295	42.056231
3505.821337	720882.306796	42.061236
3505.941450	720789.967015	42.066240
3505.759637	720705.956141	42.071245
3505.996935	720603.629011	42.076250
3505.771714	720509.607628	42.081255
3505.559435	720416.227635	42.086260
3505.538512	720338.979497	42.091264
3505.524513	720242.093991	42.096269
3505.418792	720144.379520	42.101274
3505.539980	720068.047571	42.106279
3505.287592	719973.379987	42.111284
3505.439317	719888.016648	42.116288
3505.449004	719813.386688	42.121293
3505.778473	719724.273342	42.126298
3505.335111	719635.435147	42.131303
3504.954249	719552.833895	42.136308
3505.726020	719473.959457	42.141312
3505.296471	719405.348923	42.146317
3505.316048	719304.628574	42.151322
3505.100130	719224.278039	42.156327
3505.188868	719140.603510	42.161332
3505.383486	719064.399045	42.166336
3504.793159	718985.595651	42.171341
3505.416096	718893.449547	42.176346
3505.102639	718825.658188	42.181351
3504.963393	718746.728619	42.186356
3504.995001	718666.976648	42.191360
3505.135299	718592.066269	42.196365
3504.951747	718502.528464	42.201370
3504.962336	718423.918322	42.206375
3504.974744	718348.431685	42.211380
3504.996204	718270.661441	42.216384
3504.825424	718198.030624	42.221389
3505.021252	718119.337500	42.226394
3504.672335	718052.686445	42.231399
3504.605189	717985.046068	42.236404
3504.674153	717909.446953	42.241408
3504.553069	717841.219118	42.246413
3504.753898	717770.953711	42.251418
3504.608873	717699.802304	42.256423
3504.650918	717631.347480	42.261428
3504.699189	717554.111760	42.266432
3504.328675	717488.501381	42.271437
3504.669644	717412.009741	42.276442
3504.551608	717356.475424	42.281447
3504.234326	717280.438255	42.286452
3504.512475	717209.956994	42.291456
3504.447813	717152.924453	42.296461
3504.776848	717080.796823	42.301466
3504.386751	717022.973761	42.306471
3504.848783	716949.235765	42.311476
3504.626840	716877.693217	42.316480
3504.627144	716814.992741	42.321485
3504.975093	716722.372016	42.326490
3504.651228	716651.737234	42.331495
3504.476443	716598.241091	42.336500
3504.535073	716527.194992	42.341504
3504.027049	716458.275552	42.346509
3504.494690	716392.369667	42.351514
3504.472046	716341.575232	42.356519
3504.398433	716267.076175	42.361524
3504.529676	716196.412180	42.366528
3504.480262	716139.469457	42.371533
3504.755288	716059.999825	42.376538
3504.178993	716003.391041	42.381543
3504.377973	715934.946129	42.386548
3504.520923	715865.815343	42.391552
3504.337168	715794.554936	42.396557
3504.570111	715737.364521	42.401562
3504.063770	715690.069033	42.406567
3503.984028	715610.157490	42.411572
3504.362732	715548.675132	42.416576
3503.895056	715497.998541	42.421581
3504.181963	715434.496350	42.426586
3504.513145	715364.338168	42.431591
3504.276794	715307.767911	42.436596
3504.408190	715242.751867	42.441600
3504.248569	715165.627667	42.446605
3504.231135	715112.493059	42.451610
3504.366685	715052.287521	42.456615
3504.081032	714982.227795	42.461620
3504.319299	714918.928198	42.466624
3504.048332	714873.325900	42.471629
3504.096218	714809.411836	42.476634
3503.935446	714742.852338	42.481639
3504.023730	714686.323650	42.486644
3504.107071	714619.971048	42.491648
3503.946008	714563.978805	42.496653
3504.092079	714504.164568	42.501658
3504.109263	714453.451416	42.506663
3504.001938	714389.857462	42.511668
3504.498263	714330.133139	42.516672
3503.930709	714270.087490	42.521677
3504.229543	714214.314870	42.526682
3503.946030	714145.587588	42.531687
3503.863611	714101.091322	42.536692
3504.347631	714039.431754	42.541696
3503.914046	713978.915365	42.546701
3503.821016	713912.933620	42.551706
3503.966871	713858.672524	42.556711
3503.935412	713807.516906	42.561716
3504.091182	713750.970839	42.566720
3503.893529	713709.915491	42.571725
3503.849563	713634.594301	42.576730
3503.991402	713579.885464	42.581735
3503.881682	713520.900400	42.586740
3503.934329	713472.309365	42.591744
3503.744847	713426.388072	42.596749
3503.763189	713366.735707	42.601754
3503.721616	713309.673328	42.606759
3503.677078	713259.062430	42.611764
3504.132223	713208.815533	42.616768
3503.751146	713151.708777	42.621773
3503.887469	713091.638021	42.626778
3503.799401	713047.534157	42.631783
3503.847392	712999.139683	42.636788
3503.913363	712936.895813	42.641792
3503.943143	712886.369698	42.646797
3504.327031	712810.821795	42.651802
3504.083424	712753.491187	42.656807
3503.945786	712693.363490	42.661812
3504.058191	712634.583798	42.666816
3503.520541	712583.454557	42.671821
3503.749673	712519.294799	42.676826
3503.538935	712477.491173	42.681831
3503.437158	712425.743225	42.686836
3503.767745	712376.405278	42.691840
3503.826266	712333.613585	42.696845
3503.635637	712274.732435	42.701850
3503.703432	712230.300846	42.706855
3503.600877	712176.466962	42.711860
3503.839191	712115.379840	42.716864
3503.594812	712074.572423	42.721869
3503.729273	712013.402414	42.726874
3503.641645	711963.733913	42.731879
3503.220101	711917.644143	42.736884
3503.534401	711868.157026	42.741888
3503.531013	711829.343719	42.746893
3503.876059	711767.243821	42.751898
3503.655871	711711.341714	42.756903
3503.380042	711663.638233	42.761908
3503.508323	711633.389236	42.766912
3503.516735	711581.270536	42.771917
3503.683327	711524.658205	42.776922
3503.410950	711473.031831	42.781927
3503.442477	711434.558423	42.786932
3503.408805	711387.409130	42.791937
3503.343579	711342.994819	42.796941
3502.896824	711281.865675	42.801946
3503.669214	711251.658104	42.806951
3503.294618	711200.741846	42.811956
3503.105277	711154.609672	42.816961
3503.522288	711119.347447	42.821965
3503.621306	711063.537397	42.826970
3503.331019	711017.818224	42.831975
3503.260373	710969.531008	42.836980
3503.381837	710918.580964	42.841985
3503.170601	710873.940064	42.846989
3503.318013	710830.381559	42.851994
3502.972815	710794.697539	42.856999
3502.670378	710755.630763	42.862004
3503.054353	710712.280878	42.867009
3502.922112	710674.029580	42.872013
3503.115435	710626.888312	42.877018
3502.939659	710590.579824	42.882023
3503.219148	710556.926463	42.887028
3503.305006	710516.156431	42.892033
3503.139245	710477.413353	42.897037
3503.244042	710424.278842	42.902042
3503.092457	710395.411910	42.907047
3502.986953	710353.232992	42.912052
3502.874110	710299.637136	42.917057
3502.930480	710254.551749	42.922061
3503.210178	710224.173512	42.927066
3503.269532	710183.058750	42.932071
3502.665860	710135.946802	42.937076
3503.546959	710095.192659	42.942081
3503.229984	710067.046888	42.947085
3503.249582	710011.044455	42.952090
3503.381844	709984.561963	42.957095
3503.238178	709940.103615	42.962100
3503.041946	709896.249445	42.967105
3503.260720	709854.312501	42.972109
3503.316322	709802.224785	42.977114
3503.334209	709768.412837	42.982119
3502.738257	709720.056158	42.987124
3503.155728	709677.887023	42.992129
3502.868206	709647.252669	42.997133
3502.878768	709601.674911	43.002138
3503.214148	709559.766956	43.007143
3503.044099	709536.013854	43.012148
3503.270874	709480.321336	43.017153
3503.074232	709445.252609	43.022157
3503.592271	709396.710544	43.027162
3503.652740	709351.619714	43.032167
3503.199570	709308.053101	43.037172
3503.615262	709254.860087	43.042177
3503.128811	709211.745310	43.047181
3503.183906	709174.796958	43.052186
3503.232025	709121.961582	43.057191
3503.232112	709093.561756	43.062196
3503.560972	709034.423647	43.067201
3502.899733	709009.210843	43.072205
3503.168492	708962.743073	43.077210
3502.977046	708927.969272	43.082215
3503.065159	708894.887065	43.087220
3503.353770	708837.938893	43.092225
3503.054700	708798.018514	43.097229
3502.843825	708753.813326	43.102234
3503.194640	708717.261143	43.107239
3502.783210	708672.840320	43.112244
3503.075897	708640.418561	43.117249
3502.979764	708605.925662	43.122253
3502.975281	708561.586168	43.127258
3503.216458	708520.979638	43.132263
3502.633908	708478.125260	43.137268
3502.863571	708432.753441	43.142273
3503.111344	708414.489632	43.147277
3503.101042	708372.434210	43.152282
3503.261343	708344.948935	43.157287
3503.054707	708308.039969	43.162292
3503.596129	708265.545531	43.167297
3502.968065	708221.753921	43.172301
3503.093526	708169.644754	43.177306
3503.037480	708139.413754	43.182311
3503.099237	708086.818023	43.187316
3503.157787	708052.148439	43.192321
3502.892282	708017.879705	43.197325
3502.725121	707975.053675	43.202330
3502.705287	707939.602043	43.207335
3503.061804	707904.535168	43.212340
3502.812422	707862.169036	43.217345
3502.293913	707834.645002	43.222349
3502.885126	707805.547613	43.227354
3502.903523	707762.143710	43.232359
3502.865509	707732.355225	43.237364
3503.055075	707689.270357	43.242369
3502.932467	707651.450865	43.247373
3502.794567	707615.570421	43.252378
3502.833918	707585.818339	43.257383
3503.154742	707560.737394	43.262388
3503.274056	707515.329249	43.267393
3502.852428	707478.849411	43.272397
3503.029596	707440.830619	43.277402
3503.044431	707410.337071	43.282407
3502.889003	707366.065926	43.287412
3502.940807	707327.570686	43.292417
3502.979413	707295.682320	43.297421
3502.901154	707251.745495	43.302426
3502.756648	707208.564279	43.307431
3502.825711	707179.848780	43.312436
3502.861339	707136.140905	43.317441
3502.959406	707111.492648	43.322445
3503.034145	707066.337784	43.327450
3503.011177	707028.449469	43.332455
3502.775456	706993.476463	43.337460
3503.278336	706952.869062	43.342465
3502.758289	706919.184168	43.347469
3502.889610	706877.793366	43.352474
3502.755344	706839.674242	43.357479
3502.731606	706807.198377	43.362484
3503.291205	706762.309671	43.367489
3502.850739	706734.123613	43.372493
3502.985039	706698.343478	43.377498
3503.060098	706662.175641	43.382503
3502.732697	706622.398789	43.387508
3503.106821	706582.208173	43.392513
3502.862448	706551.853620	43.397517
3503.088746	706514.517948	43.402522
3502.940168	706467.708123	43.407527
3503.075914	706434.310594	43.412532
3503.050663	706392.694930	43.417537
3503.166192	706361.187753	43.422541
3502.956327	706328.194422	43.427546
3502.982859	706283.242057	43.432551
3502.870357	706236.971364	43.437556
3503.145972	706192.523819	43.442561
3503.099307	706158.857277	43.447565
3502.927325	706132.810364	43.452570
3502.889984	706082.404062	43.457575
3502.662985	706048.915807	43.462580
3502.754358	706007.626742	43.467585
3502.698842	705976.593355	43.472589
3502.803740	705953.679048	43.477594
3502.949761	705910.592451	43.482599
3502.571193	705882.691412	43.487604
3502.757971	705849.382546	43.492609
3502.497096	705805.816110	43.497613
3502.835217	705784.899367	43.502618
3502.750094	705753.323691	43.507623
3502.492523	705716.511319	43.512628
3502.664917	705684.743951	43.517633
3502.591349	705654.606438	43.522637
3502.837112	705614.233783	43.527642
3502.925169	705585.807862	43.532647
3502.747215	705544.312604	43.537652
3502.902006	705500.676136	43.542657
3502.615353	705484.083646	43.547661
3502.914410	705442.658315	43.552666
3502.918568	705401.231705	43.557671
3502.619303	705364.226011	43.562676
3503.032101	705336.639854	43.567681
3502.783154	705308.318220	43.572685
3502.518273	705274.088113	43.577690
3502.387528	705235.861965	43.582695
3502.359181	705198.612231	43.587700
3502.923739	705162.208429	43.592705
3502.709403	705144.808602	43.597709
3503.082068	705104.213962	43.602714
3502.990200	705077.306213	43.607719
3502.577574	705045.483869	43.612724
3503.005971	705008.307077	43.617729
3502.881220	704979.616183	43.622733
3502.863981	704944.151786	43.627738
3502.992551	704900.069538	43.632743
3502.728528	704884.465653	43.637748
3502.932625	704838.632037	43.642753
3502.802238	704790.717262	43.647757
3502.724318	704761.620526	43.652762
3502.787145	704725.694963	43.657767
3502.536163	704704.375921	43.662772
3503.140188	704665.330721	43.667777
3502.872874	704633.482914	43.672781
3502.922341	704589.710174	43.677786
3503.004063	704561.083222	43.682791
3502.310644	704527.814941	43.687796
3502.829304	704477.009592	43.692801
3502.877334	704449.132975	43.697805
3502.715807	704408.225675	43.702810
3502.786689	704364.994720	43.707815
3502.591765	704350.521067	43.712820
3502.943162	704311.118477	43.717825
3502.654374	704279.471615	43.722829
3502.453563	704249.747591	43.727834
3502.639681	704212.209878	43.732839
3502.744910	704188.794054	43.737844
3503.059847	704154.662687	43.742849
3502.492730	704125.346344	43.747853
3502.357196	704091.437989	43.752858
3502.586743	704057.668063	43.757863
3502.406785	704030.970289	43.762868
3502.785847	703982.967097	43.767873
3502.541914	703957.173871	43.772877
3502.481460	703928.071454	43.777882
3502.710112	703894.350720	43.782887
3502.648295	703869.272429	43.787892
3502.637477	703835.839327	43.792897
3502.658750	703807.021120	43.797901
3502.788420	703776.297082	43.802906
3502.694853	703730.407286	43.807911
3502.257560	703707.874455	43.812916
3502.814243	703680.458046	43.817921
3502.532307	703657.700760	43.822925
3502.617821	703621.369424	43.827930
3502.332996	703591.557619	43.832935
3502.516926	703567.133509	43.837940
3502.606347	703525.534821	43.842945
3502.573003	703500.102994	43.847949
3502.435283	703470.813042	43.852954
3502.567848	703434.721585	43.857959
3502.464318	703422.218635	43.862964
3502.354614	703387.061192	43.867969
3502.566657	703367.401471	43.872973
3502.099565	703336.128320	43.877978
3502.264939	703307.483443	43.882983
3502.338336	703282.977380	43.887988
3502.787747	703250.211444	43.892993
3502.487428	703235.057715	43.897997
3502.496643	703201.320762	43.903002
3502.792042	703171.312538	43.908007
3502.689346	703135.010178	43.913012
3502.526926	703100.357106	43.918017
3502.558901	703071.981857	43.923021
3502.761683	703029.119988	43.928026
3502.795534	703005.414621	43.933031
3502.593801	702987.213407	43.938036
3502.462071	702931.537634	43.943041
3502.484353	702919.808201	43.948045
3502.628767	702882.420665	43.953050
3502.766590	702857.306553	43.958055
3502.684669	702813.695553	43.963060
3502.563509	702783.158390	43.968065
3502.589106	702755.627831	43.973069
3502.791127	702724.043473	43.978074
3502.875730	702689.745555	43.983079
3502.703109	702659.117060	43.988084
3502.937034	702611.527703	43.993089
3503.106751	702584.469732	43.998093
3502.792162	702550.435791	44.003098
3502.848545	702507.943291	44.008103
3502.978825	702474.332631	44.013108
3502.748566	702433.377648	44.018113
3502.778118	702422.391676	44.023117
3502.959538	702374.660609	44.028122
3502.946084	702336.402338	44.033127
3502.558720	702297.012963	44.038132
3502.891670	702260.734546	44.043137
3502.719323	702233.284639	44.048141
3502.805820	702197.096255	44.053146
3502.985336	702163.029071	44.058151
3502.956752	702141.816145	44.063156
3503.160051	702096.862606	44.068161
3503.020725	702056.288388	44.073165
3502.887980	702017.501771	44.078170
3502.974031	701970.231421	44.083175
3502.672987	701946.379584	44.088180
3502.901698	701899.830716	44.093185
3502.991922	701867.466605	44.098189
3503.054485	701830.634649	44.103194
3503.057699	701796.843543	44.108199
3502.845937	701763.137421	44.113204
3502.855999	701731.382323	44.118209
3502.699321	701698.809806	44.123213
3502.512731	701657.993054	44.128218
3502.845223	701624.693649	44.133223
3502.546317	701598.256455	44.138228
3502.921350	701556.352820	44.143233
3502.819577	701518.652138	44.148237
3502.893538	701477.940693	44.153242
3502.715171	701450.141448	44.158247
3502.475271	701419.221507	44.163252
3502.595209	701377.110572	44.168257
3502.685427	701361.740136	44.173261
3502.446816	701327.887668	44.178266
3502.893802	701296.506247	44.183271
3502.619225	701260.969813	44.188276
3502.782094	701222.727291	44.193281
3502.865984	701192.448931	44.198285
3502.688291	701147.950842	44.203290
3502.758964	701120.059813	44.208295
3502.358090	701094.283940	44.213300
3502.501615	701072.940660	44.218305
3502.737378	701037.915582	44.223309
3502.769568	701004.315417	44.228314
3502.724985	700969.783530	44.233319
3502.526400	700939.302351	44.238324
3502.970405	700901.658163	44.243329
3502.943054	700860.612650	44.248333
3502.609065	700828.215187	44.253338
3502.711820	700796.789298	44.258343
3502.660085	700770.805845	44.263348
3503.047639	700728.548290	44.268353
3502.783248	700700.114749	44.273357
3502.740413	700661.953366	44.278362
3503.005892	700630.897657	44.283367
3502.730787	700593.221535	44.288372
3502.724205	700561.862515	44.293377
3502.638970	700526.540385	44.298381
3502.834532	700500.167483	44.303386
3502.849368	700456.280239	44.308391
3502.751836	700426.526116	44.313396
3502.668434	700387.773819	44.318401
3502.841701	700365.131703	44.323405
3502.524413	700325.721862	44.328410
3502.559196	700295.050878	44.333415
3502.640763	700264.372078	44.338420
3502.833490	700224.331033	44.343425
3502.411172	700202.631553	44.348429
3502.483914	700162.460891	44.353434
3502.692107	700132.953603	44.358439
3502.370818	700120.183576	44.363444
3502.306548	700087.391008	44.368449
3502.421986	700062.222836	44.373453
3502.730569	700022.360586	44.378458
3502.940834	699985.794724	44.383463
3502.315662	699963.780156	44.388468
3502.533345	699930.344109	44.393473
3502.434891	699910.479247	44.398477
3502.339029	699879.828334	44.403482
3502.647678	699846.724901	44.408487
3502.652467	699823.612113	44.413492
3502.991908	699787.620581	44.418497
3502.597811	699753.539108	44.423501
3502.484163	699717.174608	44.428506
3502.755928	699681.492017	44.433511
3502.327585	699661.084493	44.438516
3502.378094	699626.183699	44.443521
3502.248085	699599.911436	44.448525
3502.390299	699582.839345	44.453530
3502.597148	699555.368232	44.458535
3502.476503	699530.585367	44.463540
3502.715733	699488.346269	44.468545
3502.779993	699449.267252	44.473549
3502.521442	699413.621246	44.478554
3503.022276	699375.116138	44.483559
3502.674934	699362.299588	44.488564
3502.719713	699319.097593	44.493569
3502.451408	699299.209624	44.498573
3502.481194	699265.006697	44.503578
3502.455409	699233.347841	44.508583
3502.312536	699209.909815	44.513588
3502.323232	699177.847092	44.518593
3502.667313	699152.787756	44.523597
3502.550460	699131.731184	44.528602
3502.738353	699083.334875	44.533607
3502.520544	699065.326946	44.538612
3502.456812	699023.881148	44.543617
3502.333801	699004.316524	44.548621
3502.616688	698972.357325	44.553626
3502.702767	698939.088309	44.558631
3502.305429	698917.431227	44.563636
3502.372161	698882.773344	44.568641
3502.540612	698854.361896	44.573645
3502.667179	698826.702895	44.578650
3502.582446	698788.987632	44.583655
3502.792736	698767.080931	44.588660
3502.659289	698732.952534	44.593665
3502.616126	698715.213366	44.598669
3502.774302	698671.343270	44.603674
3502.440442	698642.019702	44.608679
3502.630177	698612.062949	44.613684
3502.680933	698576.461993	44.618689
3502.898086	698540.236945	44.623693
3502.471200	698514.358320	44.628698
3502.924455	698475.757691	44.633703
3502.534969	698452.656544	44.638708
3502.615589	698414.266179	44.643713
3502.802704	698384.358792	44.648717
3502.310340	698364.605043	44.653722
3502.607045	698328.366014	44.658727
3502.155486	698295.779693	44.663732
3502.256436	698268.719702	44.668737
3502.482838	698245.914226	44.673741
3502.462206	698222.453420	44.678746
3502.554734	698191.169010	44.683751
3502.325510	698172.166872	44.688756
3502.200869	698128.290953	44.693761
3502.571262	698097.656409	44.698765
3502.216900	698076.537013	44.703770
3502.370623	698043.004891	44.708775
3502.242752	698037.010704	44.713780
3502.599892	698001.307221	44.718785
3502.352982	697978.728183	44.723789
3502.309190	697942.344814	44.728794
3502.838603	697911.484565	44.733799
3502.389323	697879.691752	44.738804
3502.310143	697864.591668	44.743809
3502.455730	697836.528701	44.748813
3502.223389	697798.734079	44.753818
3502.456131	697762.403830	44.758823
3502.381835	697748.396476	44.763828
3502.655984	697709.424279	44.768833
3502.715954	697688.931695	44.773837
3502.348129	697658.814989	44.778842
3502.749949	697621.064258	44.783847
3502.142959	697608.089055	44.788852
3502.633033	697574.450012	44.793857
3502.422173	697553.753158	44.798861
3502.109031	697512.639624	44.803866
3502.485651	697490.205173	44.808871
3502.383178	697459.447461	44.813876
3502.396426	697438.216239	44.818881
3502.292109	697416.457450	44.823885
3502.292687	697385.682500	44.828890
3502.529054	697362.475357	44.833895
3502.437093	697333.753887	44.838900
3502.069967	697308.458468	44.843905
3502.566765	697282.921190	44.848909
3502.540857	697258.961506	44.853914
3502.799904	697232.419178	44.858919
3502.583668	697194.718743	44.863924
3502.363814	697161.195102	44.868929
3502.508289	697142.328034	44.873933
3502.345114	697113.070674	44.878938
3502.390421	697089.645701	44.883943
3502.219894	697057.157634	44.888948
3502.277348	697032.636688	44.893953
3502.188176	697004.261718	44.898957
3502.412545	696984.535919	44.903962
3502.411463	696943.865505	44.908967
3502.535516	696933.403994	44.913972
3502.396841	696897.728020	44.918977
3502.625777	696871.736491	44.923981
3502.396481	696851.538224	44.928986
3502.326723	696817.590780	44.933991
3502.064308	696792.376064	44.938996
3502.187653	696768.291012	44.944001
3502.479931	696736.471316	44.949005
3502.316675	696716.808789	44.954010
3502.562960	696693.598255	44.959015
3502.190235	696671.235476	44.964020
3502.360416	696638.242233	44.969025
3502.601991	696614.982547	44.974029
3502.124064	696576.626483	44.979034
3502.423335	696560.666255	44.984039
3502.243880	696534.194083	44.989044
3502.306524	696504.748327	44.994049
3502.425202	696477.282137	44.999053
3502.331425	696449.353643	45.004058
3502.542834	696418.888638	45.009063
3502.425638	696407.173464	45.014068
3502.673320	696367.801921	45.019073
3502.558313	696334.804813	45.024077
3502.194531	696310.649609	45.029082
3502.619834	696268.016337	45.034087
3502.580534	696261.409662	45.039092
3502.446540	696218.967757	45.044097
3502.611575	696189.852148	45.049101
3502.434149	696166.511151	45.054106
3502.463492	696117.627428	45.059111
3502.736686	696102.963507	45.064116
3502.363955	696072.444385	45.069121
3502.714151	696043.993932	45.074125
3502.393624	696017.990979	45.079130
3502.469598	695990.231963	45.084135
3502.400021	695955.684473	45.089140
3502.356798	695933.464429	45.094145
3502.476860	695902.266814	45.099149
3502.342786	695867.132898	45.104154
3502.474568	695842.347771	45.109159
3502.165745	695815.596403	45.114164
3502.412168	695788.256202	45.119169
3502.506654	695763.477000	45.124173
3502.366916	695736.598080	45.129178
3502.229458	695701.364609	45.134183
3502.047900	695691.797341	45.139188
3502.007313	695650.232396	45.144193
3502.130815	695636.686365	45.149197
3502.317361	695626.909191	45.154202
3502.209382	695593.062793	45.159207
3501.938863	695582.416062	45.164212
3502.160859	695543.094810	45.169217
3501.937570	695522.942237	45.174221
3502.067721	695514.019604	45.179226
3502.155844	695485.162989	45.184231
3502.064207	695466.729075	45.189236
3502.048071	695426.004425	45.194241
3502.240435	695411.004581	45.199245
3502.120691	695397.597721	45.204250
3502.476220	695368.249108	45.209255
3501.824609	695352.343927	45.214260
3501.868803	695326.030196	45.219265
3502.006168	695314.669458	45.224269
3501.725424	695288.160511	45.229274
3501.888867	695258.843186	45.234279
3502.048593	695255.733740	45.239284
3502.037861	695226.743384	45.244289
3502.154009	695216.828170	45.249293
3502.017958	695195.466969	45.254298
3502.140899	695155.663023	45.259303
3502.337880	695149.016583	45.264308
3502.322017	695131.066783	45.269313
3502.282195	695104.020287	45.274317
3502.267838	695085.423655	45.279322
3502.169929	695059.182276	45.284327
3502.060008	695048.856552	45.289332
3502.281476	695019.479144	45.294337
3502.331819	694997.241332	45.299341
3502.202110	694962.351757	45.304346
3501.999427	694938.414906	45.309351
3501.853014	694909.893449	45.314356
3501.773527	694900.159311	45.319361
3502.000458	694876.549354	45.324365
3501.918730	694856.819521	45.329370
3502.067467	694839.985834	45.334375
3502.040309	694824.126001	45.339380
3501.972076	694789.175882	45.344385
3502.115957	694772.840188	45.349389
3501.807487	694751.108468	45.354394
3502.121903	694716.443138	45.359399
3502.003519	694724.817753	45.364404
3501.961081	694693.244798	45.369409
3502.319439	694670.060230	45.374413
3502.042755	694655.036929	45.379418
3502.048518	694624.898036	45.384423
3501.865443	694614.036797	45.389428
3502.483314	694580.763189	45.394433
3502.221744	694556.884743	45.399437
3502.216115	694534.207394	45.404442
3502.163322	694496.766913	45.409447
3501.952258	694498.592184	45.414452
3501.981843	694457.507416	45.419457
3502.239988	694444.086580	45.424461
3502.191734	694422.957718	45.429466
3502.600469	694399.217069	45.434471
3502.248298	694374.457847	45.439476
3502.238762	694347.901396	45.444481
3502.430495	694320.466216	45.449485
3502.007609	694302.581805	45.454490
3502.497083	694275.395833	45.459495
3501.909171	694259.328978	45.464500
3502.098580	694239.006010	45.469505
3502.101633	694212.646020	45.474509
3502.070962	694194.597294	45.479514
3502.023443	694154.717475	45.484519
3501.797287	694151.323080	45.489524
3502.352357	694137.753386	45.494529
3502.436095	694100.189264	45.499533
3501.676682	694094.445662	45.504538
3502.272727	694060.925029	45.509543
3502.193825	694046.713618	45.514548
3502.050791	694010.131466	45.519553
3502.210771	693985.734396	45.524557
3502.199998	693969.870335	45.529562
3501.704984	693938.468741	45.534567
3502.048889	693926.077463	45.539572
3501.970926	693915.993835	45.544577
3502.029001	693879.427745	45.549581
3501.957516	693878.146449	45.554586
3502.280363	693858.795366	45.559591
3502.205819	693834.386786	45.564596
3501.842862	693808.334591	45.569601
3501.771141	693781.935906	45.574605
3501.964861	693773.697377	45.579610
3501.994722	693748.525295	45.584615
3501.775642	693727.223974	45.589620
3501.980403	693711.075248	45.594625
3502.321330	693682.618758	45.599629
3502.142698	693656.535746	45.604634
3502.073169	693642.819527	45.609639
3501.884610	693617.732802	45.614644
3502.248993	693600.115159	45.619649
3502.437211	693582.576247	45.624653
3502.587203	693559.920507	45.629658
3502.191535	693522.681632	45.634663
3502.057143	693510.567544	45.639668
3502.082177	693485.196556	45.644673
3502.360419	693459.286380	45.649677
3502.456209	693440.369716	45.654682
3502.557061	693409.862856	45.659687
3502.407817	693388.897395	45.664692
3502.775074	693369.537932	45.669697
3502.454596	693319.950331	45.674701
3502.190072	693295.322874	45.679706
3502.453668	693254.044764	45.684711
3502.369641	693254.456620	45.689716
3502.476718	693232.155301	45.694721
3502.413788	693200.928604	45.699725
3502.145262	693167.994739	45.704730
3502.054469	693148.610790	45.709735
3502.108525	693128.257849	45.714740
3502.293782	693101.814803	45.719745
3502.327001	693072.859914	45.724749
3502.005186	693046.201805	45.729754
3502.511039	693028.161790	45.734759
3502.226581	693010.550412	45.739764
3502.213127	692980.458851	45.744769
3502.350576	692954.271954	45.749773
3502.223863	692929.869488	45.754778
3502.350950	692894.233082	45.759783
3502.453394	692876.010519	45.764788
3502.501684	692851.330289	45.769793
3502.591806	692820.425237	45.774797
3502.173304	692805.372427	45.779802
3502.330028	692772.516258	45.784807
3502.398689	692726.442736	45.789812
3502.294369	692643.288613	45.794817
3502.386391	692487.026604	45.799821
3501.916998	692315.234221	45.804826
3501.809913	692052.391688	45.809831
3501.717178	691764.216954	45.814836
3501.408294	691391.691472	45.819841
3501.183952	690974.358785	45.824845
3501.006393	690504.108679	45.829850
3500.656350	689966.638466	45.834855
3500.196710	689392.081540	45.839860
3499.896440	688751.771403	45.844865
3499.214027	688044.787938	45.849869
3498.405565	687293.322152	45.854874
3498.160882	686482.913339	45.859879
3497.773214	685635.716046	45.864884
3497.201481	684705.225260	45.869889
3496.905889	683726.045658	45.874893
3495.805956	682684.047633	45.879898
3495.288470	681579.628930	45.884903
3494.714716	680417.106597	45.889908
3493.534598	679204.371054	45.894913
3492.895651	677925.120570	45.899917
3491.518377	676601.963292	45.904922
3490.985189	675217.376024	45.909927
3490.197586	673774.803101	45.914932
3488.858838	672277.109153	45.919937
3487.941174	670717.825795	45.924941
3486.746941	669119.131600	45.929946
3485.875385	667446.292253	45.934951
3484.306475	665720.790668	45.939956
3483.184839	663953.438662	45.944961
3481.685994	662120.245143	45.949965
3480.729229	660259.259662	45.954970
3479.105458	658324.834148	45.959975
3477.501070	656361.757509	45.964980
3476.080163	654336.572739	45.969985
3474.731269	652259.803465	45.974989
3472.860737	650140.512024	45.979994
3471.573154	647961.498873	45.984999
3470.191149	645747.335134	45.990004
3468.511955	643481.033568	45.995009
3467.307964	641162.485268	46.000013
3465.282421	638803.377613	46.005018
3463.106226	636389.565622	46.010023
3461.261626	633939.653531	46.015028
3459.456689	631453.568087	46.020033
3457.716212	628907.449627	46.025037
3455.277905	626345.008365	46.030042
3453.613120	623729.775215	46.035047
3451.485163	621068.184091	46.040052
3449.236354	618384.157567	46.045057
3447.087054	615651.328188	46.050061
3444.624925	612884.676732	46.055066
3442.517190	610068.223718	46.060071
3440.137459	607244.234998	46.065076
3438.126153	604365.483120	46.070081
3435.635640	601454.360155	46.075085
3432.782204	598518.159658	46.080090
3430.993164	595535.089047	46.085095
3428.471659	592528.071993	46.090100
3425.826177	589478.305169	46.095105
3423.390673	586382.743126	46.100109
3420.824453	583284.348505	46.105114
3418.251103	580153.186585	46.110119
3415.506458	576977.900132	46.115124
3412.763204	573793.503043	46.120129
3410.218548	570557.037653	46.125133
3407.511109	567310.564841	46.130138
3404.779544	564027.730207	46.135143
3401.790188	560718.979360	46.140148
3399.113334	557386.576101	46.145153
3396.195530	554021.685085	46.150157
3393.062984	550647.270604	46.155162
3390.206414	547231.444131	46.160167
3387.192013	543814.496863	46.165172
3384.482354	540367.663105	46.170177
3381.197868	536896.424596	46.175181
3378.287031	533408.339062	46.180186
3375.068642	529879.491934	46.185191
3371.983046	526348.667667	46.190196
3368.469223	522793.598082	46.195201
3365.442282	519227.209223	46.200205
3362.032453	515644.242655	46.205210
3359.125451	512032.273244	46.210215
3356.071663	508421.121114	46.215220
3352.383543	504780.090565	46.220225
3349.255283	501123.085598	46.225229
3345.954109	497446.840366	46.230234
3342.748370	493757.027527	46.235239
3339.306335	490064.129751	46.240244
3335.785118	486349.608395	46.245249
3332.450247	482619.443248	46.250253
3328.929462	478878.711916	46.255258
3325.500386	475130.059664	46.260263
3322.045522	471368.246702	46.265268
3318.402636	467601.056992	46.270273
3314.935057	463799.709689	46.275277
3311.251576	460011.448867	46.280282
3307.665534	456203.649292	46.285287
3303.917388	452397.550032	46.290292
3300.096573	448576.011155	46.295297
3296.946761	444757.529980	46.300301
3292.993379	440926.183043	46.305306
3289.452787	437089.743043	46.310311
3285.691765	433248.224599	46.315316
3281.972590	429404.235458	46.320321
3278.307983	425552.507405	46.325325
3274.296045	421694.412022	46.330330
3271.014915	417830.366968	46.335335
3267.055072	413963.054131	46.340340
3263.510650	410093.372808	46.345345
3259.753986	406214.759777	46.350349
3255.799963	402351.788666	46.355354
3252.010247	398462.118043	46.360359
3248.039886	394593.580212	46.365364
3244.184259	390698.168283	46.370369
3240.631148	386817.361391	46.375373
3236.463105	382941.696675	46.380378
3232.800549	379049.574260	46.385383
3228.927399	375175.445864	46.390388
3224.893934	371299.362340	46.395393
3221.187452	367406.456185	46.400397
3217.303005	363538.989192	46.405402
3213.540072	359646.544772	46.410407
3209.145078	355770.770362	46.415412
3204.964356	351892.719169	46.420417
3201.783891	348010.774250	46.425421
3197.448148	344154.566594	46.430426
3193.749194	340292.495548	46.435431
3189.420617	336425.469858	46.440436
3185.426306	332565.000311	46.445441
3181.674601	328707.096050	46.450445
3177.434464	324850.899531	46.455450
3173.521236	320994.432440	46.460455
3169.401421	317163.737987	46.465460
3165.353247	313331.649352	46.470465
3161.564518	309498.862039	46.475469
3157.626411	305679.588188	46.480474
3153.908708	301857.842896	46.485479
3149.857509	298053.770533	46.490484
3145.739152	294243.686414	46.495489
3141.793212	290423.565927	46.500493
3137.474257	286642.813468	46.505498
3133.702844	282849.647900	46.510503
3129.724247	279065.980349	46.515508
3125.502896	275289.258320	46.520513
3121.623817	271513.184756	46.525517
3117.500686	267764.101574	46.530522
3113.489930	263997.750967	46.535527
3109.388948	260270.132831	46.540532
3105.007532	256530.940827	46.545537
3101.074225	252803.982227	46.550541
3096.783343	249086.167979	46.555546
3093.090707	245380.867400	46.560551
3088.940621	241687.808218	46.565556
3084.449093	237994.657110	46.570561
3080.679515	234319.816111	46.575565
3076.660054	230655.842214	46.580570
3072.385187	227003.002265	46.585575
3068.589570	223365.285942	46.590580
3064.568369	219725.733813	46.595585
3060.474839	216094.899622	46.600589
3056.117180	212487.822746	46.605594
3052.375366	208847.907775	46.610599
3048.338921	205188.814370	46.615604
3044.200867	201603.638893	46.620609
3040.208947	198022.983600	46.625613
3035.985036	194459.891034	46.630618
3032.006388	190905.954518	46.635623
3027.716635	187368.465619	46.640628
3023.700620	183833.235961	46.645633
3019.677058	180304.712370	46.650637
3015.386364	176792.897141	46.655642
3011.224323	173305.378685	46.660647
3007.106682	169824.250939	46.665652
3003.031145	166356.888696	46.670657
2998.915823	162901.340986	46.675661
2994.770872	159451.165018	46.680666
2991.100177	156018.152246	46.685671
2986.701042	152605.456936	46.690676
2982.573833	149196.006922	46.695681
2978.613835	145797.062899	46.700685
2974.354804	142423.608454	46.705690
2970.409385	139050.006487	46.710695
2966.205385	135694.435549	46.715700
2961.970495	132358.679541	46.720705
2958.036591	129026.738254	46.725709
2953.497169	125716.101178	46.730714
2949.132612	122415.562798	46.735719
2945.490094	119135.049219	46.740724
2941.036886	115872.592427	46.745729
2937.228744	112620.766118	46.750733
2932.895945	109386.168694	46.755738
2928.793336	106162.443357	46.760743
2924.414701	102953.245809	46.765748
2920.124639	99764.879085	46.770753
2915.903730	96592.954929	46.775757
2911.699389	93442.547868	46.780762
2907.471145	90300.231796	46.785767
2902.909922	87196.089591	46.790772
2898.512191	84093.652716	46.795777
2894.355172	81016.591984	46.800781
2889.833337	77961.319961	46.805786
2885.364990	74933.701094	46.810791
2880.963329	71929.322696	46.815796
2876.147165	68950.936559	46.820801
2871.818812	65985.592986	46.825805
2866.551516	63072.382483	46.830810
2861.479893	60178.869045	46.835815
2856.175038	57324.989483	46.840820
2850.395204	54528.180468	46.845825
2843.374148	51804.650494	46.850829
2834.423247	49213.197271	46.855834
2824.801018	46694.505509	46.860839
2816.034267	44286.561902	46.865844
2807.103851	41978.702446	46.870849
2798.554995	39784.130718	46.875853
2790.336072	37711.311320	46.880858
2782.603520	35731.258924	46.885863
2775.051370	33879.990809	46.890868
2767.570650	32119.641474	46.895873
2760.629430	30461.571852	46.900877
2753.910740	28904.146178	46.905882
2747.596775	27422.687063	46.910887
2741.628868	26038.649223	46.915892
2735.297931	24737.587233	46.920897
2729.269587	23512.103722	46.925901
2723.321337	22366.067575	46.930906
2717.597503	21293.064084	46.935911
2711.869670	20297.850026	46.940916
2706.135249	19375.419239	46.945921
2700.543897	18499.579194	46.950925
2695.369817	17705.464587	46.955930
2689.857394	16950.278150	46.960935
2684.614157	16247.520930	46.965940
2679.399584	15607.543491	46.970945
2675.022266	15006.654018	46.975949
2670.758806	14451.653219	46.980954
2666.441856	13921.894986	46.985959
2662.223827	13427.215955	46.990964
2658.177700	12982.761003	46.995969
2654.319659	12541.922580	47.000973
2650.789710	12131.186670	47.005978
2647.019435	11720.341213	47.010983
2643.851939	11334.772518	47.015988
2640.022556	10974.952895	47.020993
2637.242819	10603.890735	47.025997
2633.368238	10261.686713	47.031002
2630.645196	9906.435648	47.036007
2627.597147	9571.668722	47.041012
2624.202064	9238.554344	47.046017
2621.341155	8893.243194	47.051021
2617.881844	8562.912982	47.056026
2614.507470	8239.024009	47.061031
2611.896968	7906.498858	47.066036
2608.592958	7578.684210	47.071041
2605.227861	7238.347232	47.076045
2602.185895	6908.206616	47.081050
2599.090757	6574.136353	47.086055
2595.746855	6241.465282	47.091060
2592.407263	5909.582226	47.096065
2589.358476	5572.129888	47.101069
2586.093565	5235.454752	47.106074
2582.816005	4897.768705	47.111079
2579.266072	4563.650059	47.116084
2575.813892	4233.315449	47.121089
2572.709538	3881.762498	47.126093
2568.781008	3547.496560	47.131098
2565.529291	3217.218902	47.136103
2561.970123	2878.105611	47.141108
2558.238518	2551.484988	47.146113
2555.382950	2232.236816	47.151117
2551.124406	1903.433566	47.156122
2547.740966	1584.206034	47.161127
2544.028564	1253.769202	47.166132
2539.920849	950.269175	47.171137
2536.174627	654.473525	47.176141
2531.701311	369.877239	47.181146
2526.346023	120.153717	47.186151
2511.519478	176.023470	47.191156
2501.303010	185.784935	47.196161
2495.740192	183.848418	47.201165
2493.253989	178.789547	47.206170
2492.434257	182.622901	47.211175
2491.633724	171.230017	47.216180
2488.815231	173.668307	47.221185
2486.220124	172.403927	47.226189
2483.297645	177.652940	47.231194
2480.380796	178.411522	47.236199
2476.832373	169.809097	47.241204
2473.115208	176.870622	47.246209
2470.352555	174.290804	47.251213
2466.596012	179.624209	47.256218
2463.301081	174.254625	47.261223
2460.261886	172.135662	47.266228
2456.848241	174.861650	47.271233
2453.782320	170.206341	47.276237
2450.146992	176.466985	47.281242
2446.663226	177.061434	47.286247
2443.519825	173.135266	47.291252
2440.127655	166.061732	47.296257
2437.189307	165.157346	47.301261
2433.359819	175.067104	47.306266
2429.704213	167.924773	47.311271
2426.863310	159.940703	47.316276
2423.238894	161.712037	47.321281
2419.819664	161.030504	47.326285
2416.065404	164.504616	47.331290
2412.381225	163.331043	47.336295
2409.836432	158.059692	47.341300
2406.469261	156.635075	47.346305
2402.869694	146.703395	47.351309
2398.719161	164.964323	47.356314
2395.549164	164.473147	47.361319
2392.542274	163.090502	47.366324
2388.948247	165.659427	47.371329
2385.210420	152.940255	47.376333
2382.074394	160.285194	47.381338
2378.478982	156.589391	47.386343
2375.529223	159.606303	47.391348
2372.060899	174.280271	47.396353
2368.355020	163.957663	47.401357
2364.881117	163.797095	47.406362
2361.429727	163.396005	47.411367
2357.614834	161.288726	47.416372
2354.116548	165.008153	47.421377
2351.197774	157.206110	47.426381
2347.804988	159.574696	47.431386
2343.923764	162.831432	47.436391
2341.163039	152.176803	47.441396
2336.880738	154.795445	47.446401
2333.751339	154.774777	47.451405
2330.257983	165.217775	47.456410
2326.950916	163.704749	47.461415
2323.283107	159.393594	47.466420
2319.486679	162.787512	47.471425
2316.383961	155.083943	47.476429
2312.931248	156.494491	47.481434
2309.273605	157.355535	47.486439
2305.930326	150.707793	47.491444
2302.545502	148.158958	47.496449
2299.092355	148.588412	47.501453
2295.268108	157.143634	47.506458
2291.733253	158.521382	47.511463
2288.881247	155.861307	47.516468
2284.947558	164.597412	47.521473
2281.671067	150.022559	47.526477
2278.318278	168.809998	47.531482
2274.647282	167.689608	47.536487
2271.212994	154.972522	47.541492
2267.638198	154.332765	47.546497
2264.055777	151.912091	47.551501
2260.678689	159.749593	47.556506
2257.370330	158.326817	47.561511
2254.144924	156.682746	47.566516
2250.538644	162.149757	47.571521
2246.870241	162.456322	47.576525
2243.540398	158.018193	47.581530
2240.033187	160.828840	47.586535
2236.436171	156.554809	47.591540
2232.581373	163.477199	47.596545
2229.249077	155.694770	47.601549
2225.636922	158.000590	47.606554
2222.546556	155.947459	47.611559
2219.224318	155.209403	47.616564
2215.707270	154.433852	47.621569
2211.749411	149.592471	47.626573
2208.306876	150.392222	47.631578
2204.597574	156.952169	47.636583
2201.547343	147.696229	47.641588
2197.796930	156.384767	47.646593
2194.596770	152.027881	47.651597
2191.187152	154.568273	47.656602
2187.536014	160.736579	47.661607
2184.238623	151.043896	47.666612
2180.675855	153.706870	47.671617
2177.193818	157.375186	47.676621
2173.290219	151.653623	47.681626
2169.920858	159.682508	47.686631
2166.887514	151.143699	47.691636
2162.813895	155.473108	47.696641
2159.860678	150.330121	47.701645
2156.136365	144.603837	47.706650
2152.533222	148.578307	47.711655
2149.046293	143.342889	47.716660
2145.762198	148.552521	47.721665
2142.278731	145.300787	47.726669
2138.695165	152.415458	47.731674
2134.991172	145.620400	47.736679
2131.631818	143.941106	47.741684
2128.095006	149.440337	47.746689
2124.877418	144.747154	47.751693
2121.197689	153.288102	47.756698
2117.531614	151.360889	47.761703
2114.454168	147.281781	47.766708
2110.949902	154.835088	47.771713
2107.217485	154.657795	47.776717
2103.648614	145.783973	47.781722
2100.022455	150.257208	47.786727
2097.006499	143.583402	47.791732
2093.127691	154.600308	47.796737
2089.794694	147.608057	47.801741
2086.386772	146.271503	47.806746
2082.556057	141.199075	47.811751
2079.151235	146.041504	47.816756
2075.667984	155.022075	47.821761
2072.259536	138.903899	47.826765
2068.820665	145.082223	47.831770
2065.333382	144.616624	47.836775
2061.725033	150.605472	47.841780
2058.214704	150.694459	47.846785
2055.027454	147.061948	47.851789
2051.598015	135.023506	47.856794
2047.777968	146.284907	47.861799
2044.588462	146.180812	47.866804
2040.803872	147.554197	47.871809
2037.177188	141.782290	47.876813
2033.702751	147.046909	47.881818
2030.054431	147.427085	47.886823
2026.892117	139.202337	47.891828
2023.188554	140.990581	47.896833
2019.850243	141.162684	47.901837
2016.631456	143.548144	47.906842
2012.550105	138.819491	47.911847
2009.521389	134.027515	47.916852
2005.528953	151.431383	47.921857
2002.554863	135.662069	47.926861
1998.901971	139.411408	47.931866
1995.602194	145.513131	47.936871
1992.094680	127.670274	47.941876
1988.138013	139.011501	47.946881
1984.670431	140.046827	47.951885
1981.521592	143.857979	47.956890
1977.865528	142.493219	47.961895
1974.474677	145.798899	47.966900
1970.772073	143.474078	47.971905
1967.330707	136.112052	47.976909
1963.794339	137.425162	47.981914
1959.977079	138.952995	47.986919
1957.164130	133.932817	47.991924
1953.154363	147.055344	47.996929
1949.908245	138.604134	48.001933
1946.307104	140.703498	48.006938
1943.272795	137.280445	48.011943
1939.718866	133.635761	48.016948
1935.831962	136.656146	48.021953
1932.356191	135.886420	48.026957
1928.664430	137.155757	48.031962
1925.156783	141.318069	48.036967
1922.143372	135.985283	48.041972
1918.294180	144.415624	48.046977
1914.930763	133.176669	48.051981
1911.223613	141.039883	48.056986
1907.755319	136.085746	48.061991
1904.510724	132.049983	48.066996
1901.045769	139.132785	48.072001
1897.674122	133.772159	48.077005
1893.800513	139.758558	48.082010
1890.202924	132.437791	48.087015
1887.081627	127.386892	48.092020
1883.592386	146.578887	48.097025
1879.953710	136.643460	48.102029
1876.646818	130.502337	48.107034
1872.463155	138.522233	48.112039
1869.335342	130.431427	48.117044
1865.811220	144.723149	48.122049
1862.769438	133.141812	48.127053
1858.622860	134.635910	48.132058
1854.871048	134.647122	48.137063
1851.893511	129.016005	48.142068
1848.408246	131.921964	48.147073
1844.850025	129.652728	48.152077
1841.368318	135.506742	48.157082
1837.811073	138.436243	48.162087
1834.511828	135.665619	48.167092
1830.712377	132.558082	48.172097
1827.616777	129.326588	48.177101
1823.858928	134.252164	48.182106
1820.267987	136.864594	48.187111
1817.123314	136.838693	48.192116
1813.079562	138.978509	48.197121
1809.720491	140.823280	48.202125
1806.488961	129.407918	48.207130
1802.646627	139.679166	48.212135
1799.437217	133.885101	48.217140
1795.705914	134.805861	48.222145
1792.217632	129.713823	48.227149
1789.235037	132.263276	48.232154
1785.600540	144.500827	48.237159
1782.047698	128.660944	48.242164
1778.261800	142.673903	48.247169
1774.886779	136.411892	48.252173
1771.635141	138.633225	48.257178
1767.899859	137.203964	48.262183
1764.482527	129.126728	48.267188
1760.828972	147.160322	48.272193
1757.364459	134.622145	48.277197
1753.704447	134.783247	48.282202
1749.732945	143.122220	48.287207
1746.704447	139.486989	48.292212
1743.334272	141.347060	48.297217
1740.059113	127.487815	48.302221
1736.227150	128.281983	48.307226
1732.686697	131.036310	48.312231
1729.627711	129.050158	48.317236
1725.935956	130.602830	48.322241
1722.579800	128.820885	48.327245
1718.989211	129.409031	48.332250
1715.214249	131.618386	48.337255
1712.229457	130.522812	48.342260
1708.035946	129.809471	48.347265
1704.837399	134.437698	48.352269
1701.394642	121.404416	48.357274
1697.513042	126.407953	48.362279
1694.272914	128.408390	48.367284
1690.834934	124.719094	48.372289
1687.435467	125.714964	48.377293
1683.621956	127.433221	48.382298
1679.995525	137.815310	48.387303
1676.813656	118.340048	48.392308
1673.489860	123.748936	48.397313
1670.555403	126.217096	48.402317
1666.806419	127.359529	48.407322
1662.380149	135.083410	48.412327
1659.460848	127.983683	48.417332
1655.722391	129.050778	48.422337
1652.302786	132.706373	48.427341
1648.863970	131.843923	48.432346
1644.868436	132.366025	48.437351
1641.661277	115.836898	48.442356
1638.562902	125.417394	48.447361
1634.719388	123.800894	48.452365
1631.342575	122.225294	48.457370
1627.404048	128.168940	48.462375
1624.663206	118.688864	48.467380
1620.908663	123.209104	48.472385
1617.628691	125.666895	48.477389
1613.847049	126.131975	48.482394
1610.134996	127.607969	48.487399
1606.698840	123.697221	48.492404
1603.099128	122.299766	48.497409
1599.701260	122.904113	48.502413
1596.613909	116.578141	48.507418
1592.574100	120.186473	48.512423
1589.373389	114.620639	48.517428
1585.324967	114.888281	48.522433
1581.986995	116.312944	48.527437
1578.903089	112.461631	48.532442
1575.355806	126.509282	48.537447
1572.222351	108.548788	48.542452
1568.463554	115.827765	48.547457
1564.685905	120.297596	48.552461
1561.189707	115.541938	48.557466
1557.405030	118.793189	48.562471
1554.399170	119.482374	48.567476
1550.865260	120.602581	48.572481
1547.150160	124.346740	48.577485
1543.881863	120.417777	48.582490
1540.635673	111.022651	48.587495
1536.870179	116.897514	48.592500
1532.725237	126.179767	48.597505
1529.173706	120.370217	48.602509
1526.203906	118.929512	48.607514
1522.469884	121.028254	48.612519
1519.609325	108.702692	48.617524
1516.044823	113.867487	48.622529
1512.396130	117.673909	48.627533
1508.634330	120.408931	48.632538
1505.123575	120.402492	48.637543
1502.106376	117.110712	48.642548
1498.108439	130.363415	48.647553
1494.502373	121.960805	48.652557
1491.019944	117.818030	48.657562
1487.593715	121.037728	48.662567
1484.275779	117.614502	48.667572
1480.434651	115.406909	48.672577
1477.117378	115.530531	48.677581
1473.874755	115.356468	48.682586
1470.165902	117.661848	48.687591
1466.897111	120.212221	48.692596
1463.659196	122.571403	48.697601
1459.663866	110.468348	48.702605
1456.080547	108.612648	48.707610
1452.345259	106.595583	48.712615
1449.038422	109.576530	48.717620
1445.610642	106.235427	48.722625
1442.215991	103.888170	48.727629
1438.616105	106.947550	48.732634
1435.024766	112.677868	48.737639
1431.807866	107.267372	48.742644
1427.946359	111.636709	48.747649
1424.466871	107.314124	48.752653
1421.337945	107.121308	48.757658
1417.638341	114.567820	48.762663
1414.274995	107.765643	48.767668
1410.194698	112.411510	48.772673
1407.142069	112.326470	48.777677
1404.037833	113.731178	48.782682
1400.140237	113.173652	48.787687
1396.669555	114.366208	48.792692
1393.146020	115.420091	48.797697
1389.415144	115.012228	48.802701
1386.229434	116.663272	48.807706
1382.203564	120.240861	48.812711
1378.915693	113.142660	48.817716
1375.622406	114.061016	48.822721
1372.235880	116.499287	48.827725
1368.819117	114.019774	48.832730
1365.319813	110.999584	48.837735
1361.948615	112.900347	48.842740
1358.068772	115.214539	48.847745
1354.435470	114.617710	48.852749
1351.063199	112.248864	48.857754
1347.659688	120.904912	48.862759
1344.178917	106.576600	48.867764
1340.566556	114.864798	48.872769
1336.991584	115.579122	48.877773
1333.462063	115.588939	48.882778
1330.153057	116.776331	48.887783
1326.672102	111.777988	48.892788
1322.854081	112.491450	48.897793
1319.599060	123.580220	48.902797
1316.093396	109.784121	48.907802
1312.515798	117.548386	48.912807
1309.291406	113.675689	48.917812
1305.806558	114.623785	48.922817
1302.084411	123.494743	48.927821
1298.591806	118.773237	48.932826
1294.495194	106.246831	48.937831
1291.282468	109.101426	48.942836
1287.737327	121.736947	48.947841
1284.371459	125.892651	48.952845
1281.045555	115.243212	48.957850
1277.701276	116.989609	48.962855
1274.519559	110.107987	48.967860
1270.486466	107.236495	48.972865
1266.809025	108.812218	48.977869
1263.532386	108.221231	48.982874
1259.766449	113.360108	48.987879
1256.556530	107.910702	48.992884
1253.256665	110.754666	48.997889
1249.557759	114.556364	49.002893
1246.308406	108.598631	49.007898
1242.257125	116.938932	49.012903
1239.310877	106.562444	49.017908
1235.312690	110.760743	49.022913
1231.990879	113.803516	49.027917
1228.582120	112.408538	49.032922
1224.571740	115.966332	49.037927
1221.684307	107.465299	49.042932
1218.229889	117.599414	49.047937
1214.512383	114.217979	49.052941
1211.308934	107.034522	49.057946
1207.278093	116.988848	49.062951
1204.076693	111.727516	49.067956
1200.729511	116.584088	49.072961
1196.880883	104.234452	49.077965
1193.302131	111.868548	49.082970
1189.313220	109.602953	49.087975
1186.212517	107.001670	49.092980
1182.968388	116.919098	49.097985
1179.517102	109.919510	49.102989
1175.738912	97.349472	49.107994
1172.409475	115.388997	49.112999
1169.250602	105.215452	49.118004
1165.757478	104.719527	49.123009
1162.064127	100.264185	49.128013
1158.626860	114.554578	49.133018
1154.741313	108.025032	49.138023
1151.376725	112.252247	49.143028
1147.904711	110.229008	49.148033
1144.074697	114.683943	49.153037
1141.047478	104.264875	49.158042
1137.343879	109.997983	49.163047
1134.289965	112.606791	49.168052
1130.602893	117.081321	49.173057
1126.768268	112.111816	49.178061
1123.714741	115.773756	49.183066
1119.901973	110.006955	49.188071
1116.329515	98.291370	49.193076
1112.748251	115.873104	49.198081
1109.219364	111.071518	49.203085
1106.140328	112.254199	49.208090
1102.152917	115.571890	49.213095
1098.809564	110.197354	49.218100
1095.134090	118.800455	49.223105
1091.946184	117.452933	49.228109
1088.586977	104.139398	49.233114
1084.541505	111.414625	49.238119
1081.362821	108.928926	49.243124
1077.775397	109.319509	49.248129
1074.502764	110.960075	49.253133
1071.314069	107.830747	49.258138
1067.442944	104.690332	49.263143
1063.967164	109.481826	49.268148
1060.064847	114.281098	49.273153
1056.572372	120.544732	49.278157
1053.426608	104.798290	49.283162
1049.694392	110.331558	49.288167
1046.597726	108.184174	49.293172
1042.674604	110.508940	49.298177
1039.278497	112.385046	49.303181
1035.834510	110.361997	49.308186
1032.202248	116.964895	49.313191
1028.866296	112.982981	49.318196
1025.473752	114.121652	49.323201
1021.736479	121.691706	49.328205
1018.380946	116.884222	49.333210
1014.452930	112.291783	49.338215
1010.976002	109.699556	49.343220
1007.721041	113.115844	49.348225
1004.317169	112.093000	49.353229
1001.324948	114.150793	49.358234
997.428612	106.102501	49.363239
993.885653	106.235378	49.368244
989.900057	112.863581	49.373249
986.521128	112.586506	49.378253
983.450236	102.556433	49.383258
979.732199	113.747818	49.388263
976.216936	107.336388	49.393268
972.777463	107.078610	49.398273
969.122756	119.261213	49.403277
965.530419	111.560508	49.408282
962.147103	119.357619	49.413287
959.077541	104.659737	49.418292
955.484230	112.728775	49.423297
951.657759	117.521711	49.428301
948.372902	102.869508	49.433306
944.257798	115.367830	49.438311
941.193039	112.266449	49.443316
937.594295	118.186812	49.448321
934.283408	115.245528	49.453325
931.021084	111.620535	49.458330
927.488424	112.544068	49.463335
923.941626	115.870936	49.468340
920.151406	112.169268	49.473345
916.297664	109.864793	49.478349
913.356959	105.218690	49.483354
909.305241	104.779629	49.488359
906.231388	101.670899	49.493364
902.786835	106.592125	49.498369
899.232957	113.845603	49.503373
896.217803	101.761580	49.508378
892.091717	111.123712	49.513383
888.572498	105.231810	49.518388
884.522366	106.304304	49.523393
881.416408	104.936871	49.528397
878.576315	109.068848	49.533402
874.958681	117.263528	49.538407
871.461015	109.437728	49.543412
867.732969	118.708596	49.548417
864.276616	117.582846	49.553421
860.926731	109.143169	49.558426
857.097548	104.598864	49.563431
853.695133	109.774233	49.568436
849.948914	104.257947	49.573441
846.083052	102.962154	49.578445
843.282404	103.928272	49.583450
839.788542	111.049318	49.588455
836.402369	107.219130	49.593460
832.938155	110.825256	49.598465
829.130737	109.399632	49.603469
825.339309	102.021873	49.608474
821.938375	107.166827	49.613479
818.546602	103.348237	49.618484
814.935046	104.036066	49.623489
811.613222	109.109333	49.628493
808.325829	94.870511	49.633498
804.756019	109.229018	49.638503
801.061396	101.630435	49.643508
797.382717	104.999143	49.648513
794.023722	109.081628	49.653517
790.995775	104.180679	49.658522
787.082686	112.812056	49.663527
783.747619	105.827127	49.668532
780.236716	107.638742	49.673537
776.488893	104.514503	49.678541
773.112277	100.575042	49.683546
769.258319	121.692582	49.688551
766.045014	110.398615	49.693556
762.434115	112.528511	49.698561
759.026175	103.959405	49.703565
755.714039	106.386605	49.708570
752.037070	105.552003	49.713575
748.408192	103.570819	49.718580
745.169723	107.225310	49.723585
741.332650	105.610885	49.728589
738.276139	111.492414	49.733594
734.635626	107.986572	49.738599
731.027698	106.432919	49.743604
727.700368	107.158853	49.748609
724.111527	106.277135	49.753613
720.610099	104.365468	49.758618
716.800587	113.974342	49.763623
713.356284	103.579813	49.768628
709.876344	112.934270	49.773633
706.361349	104.083165	49.778637
703.114771	105.950373	49.783642
699.451714	109.462801	49.788647
696.222006	98.481828	49.793652
692.346827	100.056584	49.798657
688.360152	101.377070	49.803661
685.637053	91.365682	49.808666
682.113613	103.268444	49.813671
678.911316	103.720745	49.818676
675.407567	98.831897	49.823681
671.691884	107.695728	49.828685
668.192181	99.302515	49.833690
664.167576	106.616669	49.838695
660.577265	107.045558	49.843700
657.380808	100.689803	49.848705
653.550279	100.097759	49.853709
650.811259	108.933822	49.858714
646.829381	102.976589	49.863719
643.511135	106.161468	49.868724
640.139444	101.854255	49.873729
636.277869	104.431643	49.878733
633.164444	101.294139	49.883738
629.069046	106.551362	49.888743
625.560327	105.574181	49.893748
622.259099	99.949356	49.898753
619.160294	104.879297	49.903757
615.832278	106.178097	49.908762
611.854578	108.736042	49.913767
608.492328	115.112639	49.918772
604.985075	110.615941	49.923777
601.218474	104.252735	49.928781
597.392269	103.146951	49.933786
594.050425	108.060880	49.938791
591.000878	108.566907	49.943796
587.771115	105.365606	49.948801
584.172114	108.671376	49.953805
580.894428	102.087385	49.958810
576.905601	106.350998	49.963815
573.218133	106.910883	49.968820
569.512386	102.405028	49.973825
566.249915	113.761885	49.978829
562.875219	106.006785	49.983834
558.983008	105.955271	49.988839
555.727542	98.657809	49.993844
552.621733	100.593791	49.998849
548.998714	100.818415	50.003853
545.354983	103.996836	50.008858
541.668183	105.838530	50.013863
538.500612	100.713018	50.018868
535.209929	107.429474	50.023873
531.271556	103.215326	50.028877
528.075531	103.007006	50.033882
524.194138	116.604040	50.038887
520.976108	108.567699	50.043892
517.387124	106.482823	50.048897
513.744070	109.637675	50.053901
510.278746	104.950205	50.058906
506.463358	104.912665	50.063911
503.350418	99.428463	50.068916
499.670313	104.179192	50.073921
496.216816	110.853352	50.078925
493.084330	101.116058	50.083930
489.606162	106.093862	50.088935
486.228551	101.969501	50.093940
482.587863	106.856789	50.098945
478.854489	110.272101	50.103949
475.314784	102.806249	50.108954
471.625863	104.342679	50.113959
468.282133	111.444871	50.118964
464.864848	108.114657	50.123969
461.093803	111.483726	50.128973
457.448197	98.817862	50.133978
453.830108	107.563093	50.138983
450.248280	99.144790	50.143988
447.434668	99.545370	50.148993
443.953262	100.077184	50.153997
440.630268	91.473979	50.159002
436.829028	114.788620	50.164007
433.152556	106.397041	50.169012
429.982288	102.432394	50.174017
426.253324	102.484618	50.179021
422.762567	89.466975	50.184026
418.906766	98.776873	50.189031
415.615751	101.896829	50.194036
412.430819	99.166785	50.199041
408.641616	108.545004	50.204045
405.487236	94.166329	50.209050
401.596283	96.755292	50.214055
398.290944	99.806590	50.219060
394.569464	98.847444	50.224065
391.063036	107.180360	50.229069
387.738057	101.843425	50.234074
384.163772	106.181668	50.239079
380.676866	106.083166	50.244084
377.635059	101.341899	50.249089
373.745061	93.021244	50.254093
370.344618	99.043397	50.259098
366.331070	96.670755	50.264103
362.851152	95.500173	50.269108
359.631828	87.405188	50.274113
356.048593	99.777659	50.279117
352.710553	93.469266	50.284122
349.108628	96.735054	50.289127
345.952398	93.380284	50.294132
342.436439	95.225638	50.299137
338.443701	102.187876	50.304141
335.049046	95.528928	50.309146
331.386555	102.872623	50.314151
328.227615	99.791426	50.319156
324.608689	94.838668	50.324161
321.144321	98.769424	50.329165
317.672437	98.337950	50.334170
314.023084	109.076810	50.339175
310.736324	99.809207	50.344180
307.133112	96.265402	50.349185
303.347484	98.918715	50.354189
300.409895	87.262412	50.359194
296.759821	96.923354	50.364199
293.110894	93.274846	50.369204
289.708029	92.085058	50.374209
286.208187	98.147997	50.379213
282.754892	88.232316	50.384218
279.038335	104.246234	50.389223
275.229983	99.679090	50.394228
271.910355	86.421723	50.399233
268.401590	99.508516	50.404237
265.211594	94.323984	50.409242
261.563103	94.391448	50.414247
257.981449	99.928437	50.419252
254.783518	97.454044	50.424257
251.152751	105.580905	50.429261
248.151241	99.601892	50.434266
244.045329	106.226559	50.439271
240.099772	103.904350	50.444276
237.140284	92.814716	50.449281
233.338482	104.221390	50.454285
230.252775	91.831497	50.459290
226.367390	108.303198	50.464295
222.591122	104.430147	50.469300
219.590146	102.081243	50.474305
215.984660	104.720400	50.479309
213.003969	99.979994	50.484314
209.061968	99.753714	50.489319
205.566164	103.147684	50.494324
201.792224	101.563551	50.499329
198.596622	104.349766	50.504333
195.385332	93.068205	50.509338
191.539128	103.378765	50.514343
188.215427	94.750240	50.519348
184.588476	98.266380	50.524353
180.466674	96.706110	50.529357
177.397640	100.984354	50.534362
173.640856	99.469434	50.539367
170.489564	95.277282	50.544372
166.951502	99.887940	50.549377
163.721120	100.674621	50.554381
159.907529	105.526657	50.559386
156.145181	102.783473	50.564391
152.827739	101.715025	50.569396
149.580418	103.612359	50.574401
146.560845	104.982601	50.579405
142.924942	99.722802	50.584410
138.891450	102.342700	50.589415
135.579279	103.392374	50.594420
132.035316	98.840794	50.599425
128.361127	104.866809	50.604429
124.910449	99.651152	50.609434
121.475367	96.665957	50.614439
117.937745	93.186842	50.619444
114.566180	95.908911	50.624449
110.650973	93.392558	50.629453
107.345464	90.457753	50.634458
103.934126	98.895702	50.639463
100.631793	88.946905	50.644468
97.166931	97.117057	50.649473
93.377242	102.868589	50.654477
89.841718	92.616229	50.659482
86.377092	99.160314	50.664487
82.610713	98.743456	50.669492
79.784949	89.563126	50.674497
75.834632	92.678432	50.679501
72.222965	93.761167	50.684506
68.791364	94.145916	50.689511
65.340567	97.495049	50.694516
61.881667	98.355164	50.699521
57.991728	94.086490	50.704525
54.920167	95.771074	50.709530
51.625370	93.434437	50.714535
47.733531	98.156060	50.719540
44.225198	89.074371	50.724545
41.009551	96.317267	50.729549
37.698968	92.724853	50.734554
33.854148	98.155223	50.739559
30.451753	91.753174	50.744564
27.194900	86.041381	50.749569
22.931659	104.543022	50.754573
19.427570	87.890505	50.759578
16.038505	90.024530	50.764583
12.798681	91.861128	50.769588
9.510888	101.889728	50.774593
5.967207	91.134412	50.779597
2.552583	97.553654	50.784602