Tue Jun 21 10:52:40 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
0.113050	79.071827	0.000000
0.134360	88.322749	0.005005
-0.035422	103.238823	0.010010
0.216704	109.613079	0.015014
0.324871	95.952123	0.020019
0.134228	82.056102	0.025024
0.306176	78.528370	0.030029
-0.511388	81.392752	0.035034
-0.444730	72.122075	0.040038
-0.599630	68.007329	0.045043
-1.193580	64.206034	0.050048
-1.307790	49.587181	0.055053
-1.628834	53.618660	0.060058
-2.117461	41.125927	0.065062
-2.702355	25.528513	0.070067
-2.860626	22.368643	0.075072
-2.593118	23.012911	0.080077
-2.801187	31.050490	0.085082
-3.499392	11.645359	0.090086
-3.769759	10.823509	0.095091
-3.785583	11.126144	0.100096
-3.862905	8.388781	0.105101
-4.031359	14.904076	0.110106
-4.712724	2.916890	0.115110
-4.467452	4.001142	0.120115
-5.365630	-2.975761	0.125120
-5.396497	-5.134142	0.130125
-6.254668	2.717836	0.135130
-6.451134	-1.382903	0.140134
-6.521851	-8.053613	0.145139
-7.007883	5.591024	0.150144
-7.011982	5.390491	0.155149
-7.103545	9.528012	0.160154
-6.801096	6.448340	0.165158
-7.390831	9.080216	0.170163
-8.218337	15.557630	0.175168
-8.043990	13.175825	0.180173
-8.413634	5.514663	0.185178
-8.314101	8.762141	0.190182
-8.160384	12.385841	0.195187
-9.156460	4.170107	0.200192
-9.377569	8.642445	0.205197
-9.643318	13.304907	0.210202
-9.526553	15.056903	0.215206
-10.065147	15.014733	0.220211
-11.171816	13.277213	0.225216
-10.471643	13.314272	0.230221
-11.071297	15.649621	0.235226
-11.450410	12.757598	0.240230
-11.605058	13.389482	0.245235
-11.363710	19.766076	0.250240
-11.639766	11.919904	0.255245
-11.779142	17.543371	0.260250
-11.888460	7.031048	0.265254
-12.661279	13.471384	0.270259
-13.247544	10.557424	0.275264
-12.974700	8.844451	0.280269
-13.188221	14.293517	0.285274
-13.182873	12.245761	0.290278
-13.992992	10.641472	0.295283
-14.789786	5.474493	0.300288
-14.564991	2.083068	0.305293
-14.777468	7.870977	0.310298
-14.663354	2.126921	0.315302
-14.700522	0.249204	0.320307
-14.867099	6.174750	0.325312
-15.210007	-5.213524	0.330317
-16.014028	-2.617600	0.335322
-16.136197	0.272711	0.340326
-16.397493	-1.155070	0.345331
-16.394647	10.496261	0.350336
-16.788311	11.447938	0.355341
-17.358141	7.626880	0.360346
-17.090144	-0.496646	0.365350
-17.409218	7.947655	0.370355
-17.773029	-1.488494	0.375360
-17.686528	-2.795479	0.380365
-18.527118	8.239732	0.385370
-18.969848	4.592001	0.390374
-18.804425	7.723585	0.395379
-19.122770	11.232266	0.400384
-18.994643	3.429282	0.405389
-19.520202	12.131947	0.410394
-20.094892	5.139365	0.415398
-20.728937	12.968247	0.420403
-20.595604	9.741938	0.425408
-20.205222	-3.546920	0.430413
-20.591559	9.011074	0.435418
-20.711729	-4.226787	0.440422
-21.243582	-1.962655	0.445427
-21.860443	3.490643	0.450432
-22.135640	-0.195485	0.455437
-22.371385	4.103649	0.460442
-22.326222	7.253569	0.465446
-22.455063	0.762978	0.470451
-22.581614	6.784311	0.475456
-23.052542	5.603179	0.480461
-23.521619	11.209411	0.485466
-23.820115	7.350526	0.490470
-23.842118	8.387474	0.495475
-24.004186	12.929364	0.500480
-23.809248	8.730657	0.505485
-24.891818	11.525842	0.510490
-25.069552	6.564785	0.515494
-25.293454	2.515554	0.520499
-25.269080	2.643010	0.525504
-25.356725	-4.895136	0.530509
-25.742595	5.056403	0.535514
-25.765877	-0.598793	0.540518
-26.682755	5.586960	0.545523
-26.866563	1.200755	0.550528
-26.751692	4.846080	0.555533
-27.098321	9.359726	0.560538
-27.121027	0.277152	0.565542
-27.430740	5.112651	0.570547
-28.366478	3.451024	0.575552
-28.479854	0.384366	0.580557
-28.829003	8.721955	0.585562
-28.837606	5.119355	0.590566
-28.686695	-0.140026	0.595571
-28.650524	-4.463004	0.600576
-28.881152	4.563186	0.605581
-29.703764	7.938699	0.610586
-30.150866	3.928008	0.615590
-30.215576	10.545112	0.620595
-30.261003	6.164012	0.625600
-29.968619	-1.545007	0.630605
-30.744652	7.652211	0.635610
-31.250525	10.233104	0.640614
-31.570640	-0.481894	0.645619
-31.851992	-5.045725	0.650624
-31.730501	0.388905	0.655629
-32.279840	-5.957655	0.660634
-32.101510	5.723614	0.665638
-32.940870	9.249507	0.670643
-33.398954	1.116372	0.675648
-33.435104	0.899243	0.680653
-33.559688	15.138390	0.685658
-33.699246	3.485165	0.690662
-33.513534	9.094064	0.695667
-33.457668	4.971076	0.700672
-33.891595	0.190579	0.705677
-34.807555	6.010129	0.710682
-35.178178	4.716682	0.715686
-35.291243	-0.732233	0.720691
-35.424637	7.041959	0.725696
-35.281540	0.509100	0.730701
-35.922977	2.046448	0.735706
-36.524791	0.441611	0.740710
-36.796278	-1.798086	0.745715
-36.494681	9.435941	0.750720
-36.807249	-2.150149	0.755725
-36.867961	5.444273	0.760730
-37.188190	-0.606340	0.765734
-38.071610	0.680408	0.770739
-38.581389	5.376964	0.775744
-38.810748	2.912829	0.780749
-38.251877	11.047169	0.785754
-38.186186	1.944035	0.790758
-38.230527	9.345125	0.795763
-38.771027	0.824461	0.800768
-39.492101	1.916198	0.805773
-40.167381	4.576450	0.810778
-40.308287	13.192528	0.815782
-40.150797	4.981333	0.820787
-40.561055	7.828776	0.825792
-40.427659	0.648692	0.830797
-40.450177	7.584012	0.835802
-40.910933	3.849878	0.840806
-41.570269	5.373220	0.845811
-41.954560	11.708174	0.850816
-41.750242	4.131939	0.855821
-42.028232	3.129808	0.860826
-42.062762	5.253570	0.865830
-42.739266	4.991720	0.870835
-43.116712	17.257773	0.875840
-42.934179	2.099657	0.880845
-43.386179	8.759582	0.885850
-43.265113	-2.112535	0.890854
-43.588124	5.657338	0.895859
-44.700027	8.987225	0.900864
-44.664554	4.757305	0.905869
-45.200076	3.746515	0.910874
-45.133669	1.224324	0.915878
-44.935473	8.671681	0.920883
-45.169440	5.211974	0.925888
-45.173934	8.807209	0.930893
-45.948779	4.484545	0.935898
-46.392287	7.238631	0.940902
-46.440766	-4.336330	0.945907
-46.533628	10.749050	0.950912
-46.458244	5.490729	0.955917
-47.391294	1.834019	0.960922
-48.045757	15.506358	0.965926
-47.978398	1.953085	0.970931
-48.244878	11.010474	0.975936
-47.720558	1.459222	0.980941
-48.078788	10.513649	0.985946
-48.158146	-0.292916	0.990950
-48.960832	-0.442899	0.995955
-49.358193	4.628128	1.000960
-49.578019	2.442629	1.005965
-49.921320	7.098198	1.010970
-50.053054	0.550073	1.015974
-49.790368	1.355962	1.020979
-50.348418	7.658516	1.025984
-50.875357	4.215950	1.030989
-51.444361	8.584876	1.035994
-51.204154	3.499160	1.040998
-51.453750	6.796360	1.046003
-51.644749	6.955140	1.051008
-51.388633	8.125407	1.056013
-52.184944	4.412309	1.061018
-52.216340	-2.683257	1.066022
-52.726010	-3.840011	1.071027
-53.037528	4.439643	1.076032
-52.710065	-3.428117	1.081037
-53.240175	8.491435	1.086042
-53.942528	0.166298	1.091046
-54.110312	-4.485404	1.096051
-54.857007	1.970735	1.101056
-54.387862	-7.101327	1.106061
-54.926357	1.552761	1.111066
-54.312498	3.946252	1.116070
-54.627760	-3.507035	1.121075
-55.397319	-4.909252	1.126080
-55.838371	-3.601235	1.131085
-56.051070	-0.914577	1.136090
-56.095607	-5.035143	1.141094
-55.892160	-4.925108	1.146099
-57.034649	-3.705763	1.151104
-57.269798	3.279763	1.156109
-57.613836	0.128761	1.161114
-57.785461	-3.171165	1.166118
-57.579834	-3.171406	1.171123
-57.889095	2.979638	1.176128
-57.508359	-1.892943	1.181133
-58.150541	8.250424	1.186138
-58.815113	0.871953	1.191142
-58.952616	-3.316690	1.196147
-59.481136	13.253741	1.201152
-59.021657	-10.270382	1.206157
-59.476213	3.521776	1.211162
-60.578951	4.306326	1.216166
-60.675241	-0.009910	1.221171
-60.838300	-1.584394	1.226176
-60.835227	0.452431	1.231181
-60.947503	12.369095	1.236186
-60.692616	0.999243	1.241190
-60.854852	2.012645	1.246195
-61.558463	3.311258	1.251200
-62.197247	-4.453122	1.256205
-62.480285	3.201795	1.261210
-62.398456	5.743578	1.266214
-62.283760	5.141927	1.271219
-63.132273	5.507275	1.276224
-63.825816	0.511467	1.281229
-63.436355	7.004022	1.286234
-63.474068	5.009772	1.291238
-64.033942	1.042232	1.296243
-63.803573	10.516395	1.301248
-63.989420	5.128669	1.306253
-65.029733	7.559100	1.311258
-65.651283	2.461188	1.316262
-65.334048	5.260776	1.321267
-65.945454	12.595341	1.326272
-65.617350	3.080529	1.331277
-66.040856	14.270650	1.336282
-65.659654	7.706054	1.341286
-66.058519	1.054169	1.346291
-66.819682	10.977087	1.351296
-66.744223	2.397245	1.356301
-67.253428	12.104786	1.361306
-67.128797	3.476741	1.366310
-67.313615	4.842571	1.371315
-68.526051	11.183444	1.376320
-68.648760	10.794959	1.381325
-68.578419	5.495640	1.386330
-69.007687	9.449918	1.391334
-68.530165	0.409616	1.396339
-68.677579	10.931624	1.401344
-69.189021	5.824950	1.406349
-70.048987	8.255905	1.411354
-70.312098	6.509339	1.416358
-70.199609	-1.301311	1.421363
-70.674340	9.232672	1.426368
-70.475939	2.902393	1.431373
-70.315442	8.627943	1.436378
-71.337930	14.785613	1.441382
-71.578295	-0.653914	1.446387
-71.985101	14.973831	1.451392
-71.339046	8.753330	1.456397
-71.931838	6.451405	1.461402
-72.951476	13.098383	1.466406
-73.315772	3.623644	1.471411
-73.638008	13.820393	1.476416
-73.201733	10.378353	1.481421
-73.514959	13.314514	1.486426
-74.003974	5.244129	1.491430
-73.610117	1.205671	1.496435
-73.892309	2.494881	1.501440
-74.441645	4.661471	1.506445
-74.673449	8.212851	1.511450
-75.414270	0.152596	1.516454
-75.081726	-3.017111	1.521459
-75.348167	3.808627	1.526464
-75.279951	7.156204	1.531469
-75.656220	4.646546	1.536474
-76.522922	7.108414	1.541478
-77.014345	0.463176	1.546483
-77.170519	10.848896	1.551488
-77.181465	-3.897302	1.556493
-77.066605	15.047254	1.561498
-77.137309	11.921039	1.566502
-77.103597	7.473950	1.571507
-77.988749	10.424315	1.576512
-78.195623	0.492533	1.581517
-78.604671	7.718599	1.586522
-78.547693	2.208572	1.591526
-79.212066	8.072502	1.596531
-79.687572	11.191628	1.601536
-79.686579	7.112657	1.606541
-79.993667	11.311325	1.611546
-80.096891	1.862026	1.616550
-79.718874	5.825874	1.621555
-80.356608	12.551687	1.626560
-80.775967	-0.379691	1.631565
-81.205023	10.650521	1.636570
-81.518948	5.400829	1.641574
-81.499758	11.454266	1.646579
-81.731025	9.413137	1.651584
-81.346206	7.220055	1.656589
-82.079038	13.620428	1.661594
-82.932083	12.695379	1.666598
-82.804103	6.642963	1.671603
-83.351818	13.106018	1.676608
-83.201643	6.335186	1.681613
-83.407654	6.608736	1.686618
-83.562838	12.307436	1.691622
-83.437817	1.153268	1.696627
-84.602977	2.177857	1.701632
-84.874923	0.751055	1.706637
-85.051659	6.196000	1.711642
-85.167178	-1.872692	1.716646
-85.445636	-0.140694	1.721651
-85.469806	7.067414	1.726656
-84.971160	-9.445436	1.731661
-85.978773	2.423739	1.736666
-86.433394	2.684195	1.741670
-86.483319	6.739831	1.746675
-86.541218	6.583334	1.751680
-86.741349	2.746844	1.756685
-87.573194	4.881684	1.761690
-87.935262	4.539943	1.766694
-87.758519	4.475221	1.771699
-88.411285	5.587424	1.776704
-87.901798	9.377948	1.781709
-88.493939	6.497140	1.786714
-88.492627	2.254330	1.791718
-88.933162	2.588821	1.796723
-89.786398	4.241962	1.801728
-89.566212	0.016383	1.806733
-89.699758	4.248666	1.811738
-90.037157	5.835521	1.816742
-89.823729	0.666427	1.821747
-90.494861	2.778400	1.826752
-90.934385	0.312175	1.831757
-91.506921	3.206821	1.836762
-91.813270	4.401365	1.841766
-91.560467	0.592677	1.846771
-91.797410	3.977174	1.851776
-91.620965	5.637389	1.856781
-91.677379	6.428238	1.861786
-92.717744	3.124778	1.866790
-93.029376	1.782297	1.871795
-93.366091	8.093783	1.876800
-93.194459	9.056434	1.881805
-93.426656	0.461439	1.886810
-93.435366	5.653202	1.891814
-93.950337	4.729196	1.896819
-94.505387	12.456397	1.901824
-94.648070	2.742893	1.906829
-94.739105	15.735450	1.911834
-94.687501	10.055025	1.916838
-94.857303	1.495478	1.921843
-95.859986	11.414985	1.926848
-96.141652	8.130520	1.931853
-96.314474	7.023557	1.936858
-96.262314	2.097646	1.941862
-96.326806	-3.400352	1.946867
-96.558715	5.785887	1.951872
-96.469662	1.828888	1.956877
-97.368308	4.291314	1.961882
-97.835601	5.267426	1.966886
-97.858740	4.526986	1.971891
-98.036579	14.539586	1.976896
-98.069880	-0.837336	1.981901
-98.581136	6.049864	1.986906
-99.041884	3.505261	1.991910
-99.228994	7.757862	1.996915
-99.647364	6.548407	2.006912
-98.671375	1.808650	2.016909
-97.942864	2.882540	2.026906
-98.273241	3.417919	2.036902
-97.961028	2.814491	2.046899
-97.000876	6.408754	2.056896
-96.742727	2.951066	2.066893
-95.872071	6.519251	2.076890
-95.338759	1.380379	2.086886
-95.159343	-4.022539	2.096883
-94.712334	6.760108	2.106880
-94.124828	4.289151	2.116877
-93.757412	5.471055	2.126874
-92.748937	1.145986	2.136870
-92.580027	5.905452	2.146867
-92.079946	3.467547	2.156864
-91.356716	8.107550	2.166861
-91.116557	5.687005	2.176858
-90.485370	3.594305	2.186854
-89.785120	8.512363	2.196851
-89.408839	10.992519	2.206848
-89.255366	2.677134	2.216845
-88.599469	7.622691	2.226842
-88.073430	4.901299	2.236838
-87.407595	2.474672	2.246835
-86.464436	9.511126	2.256832
-86.206203	9.469879	2.266829
-86.101730	4.059413	2.276826
-85.809747	1.190461	2.286822
-84.707698	1.361173	2.296819
-84.609190	1.470066	2.306816
-84.257700	5.379315	2.316813
-83.308684	9.007436	2.326810
-82.988872	6.530823	2.336806
-82.380986	6.514262	2.346803
-81.572614	0.268211	2.356800
-81.626774	0.707855	2.366797
-81.434663	4.563872	2.376794
-80.620237	6.747010	2.386790
-80.151359	11.647669	2.396787
-79.120746	2.376131	2.406784
-78.690326	0.287636	2.416781
-78.573666	3.932876	2.426778
-78.280279	3.114433	2.436774
-77.332341	9.386628	2.446771
-77.031730	10.424690	2.456768
-76.419242	9.547079	2.466765
-75.882742	3.189366	2.476762
-75.687829	8.889382	2.486758
-74.633664	6.526482	2.496755
-74.145234	3.903790	2.506752
-73.999498	9.891337	2.516749
-73.779176	6.209331	2.526746
-72.952518	3.032513	2.536742
-72.445610	8.894649	2.546739
-72.126131	12.072208	2.556736
-71.068289	7.050182	2.566733
-70.940110	10.207653	2.576730
-70.773333	5.754050	2.586726
-69.863112	12.926175	2.596723
-69.733418	2.592634	2.606720
-68.853655	6.648934	2.616717
-67.940284	6.824618	2.626714
-67.818993	7.624055	2.636710
-67.593612	4.289556	2.646707
-67.255554	7.806453	2.656704
-66.432140	5.752657	2.666701
-66.080840	8.406086	2.676698
-64.859749	7.261915	2.686694
-64.728628	7.888615	2.696691
-64.910489	6.311902	2.706688
-64.040771	3.870482	2.716685
-63.198432	0.682375	2.726682
-63.065642	-4.735939	2.736678
-62.368412	-0.189431	2.746675
-61.751296	9.279364	2.756672
-61.607052	3.144284	2.766669
-60.801604	5.316861	2.776666
-60.388583	-2.337705	2.786662
-59.885789	0.855533	2.796659
-59.667114	5.778067	2.806656
-58.619447	7.649916	2.816653
-58.328486	8.640577	2.826650
-58.063036	5.087432	2.836646
-57.018069	-1.732463	2.846643
-56.722809	9.066432	2.856640
-56.612949	4.798897	2.866637
-56.261744	-0.372054	2.876634
-55.431070	4.574994	2.886630
-54.961707	5.966848	2.896627
-54.151378	6.870315	2.906624
-53.708479	6.128475	2.916621
-53.661049	5.900646	2.926618
-53.116287	2.173409	2.936614
-52.213899	4.718585	2.946611
-52.084638	0.819695	2.956608
-50.935895	-0.949310	2.966605
-50.569071	3.831128	2.976602
-50.622234	1.465086	2.986598
-50.233185	-5.028446	2.996595
-49.069793	-0.494719	3.006592
-48.747704	7.113862	3.016589
-48.785889	-3.227442	3.026586
-47.714483	2.138733	3.036582
-47.219123	0.011825	3.046579
-47.138865	-0.032351	3.056576
-46.107540	1.758628	3.066573
-45.578398	-1.626173	3.076570
-45.510902	2.625500	3.086566
-45.303598	-8.794371	3.096563
-44.686520	-6.212815	3.106560
-43.867193	1.931667	3.116557
-42.906819	3.414703	3.126554
-42.617617	-0.889643	3.136550
-42.759535	-0.622382	3.146547
-41.910115	1.621555	3.156544
-41.002960	5.034729	3.166541
-41.231636	-0.529021	3.176538
-40.094727	-1.536149	3.186534
-39.671091	0.082796	3.196531
-39.654749	-0.397932	3.206528
-39.355149	-6.687758	3.216525
-38.487976	-2.995889	3.226522
-37.510346	-3.931393	3.236518
-36.768365	1.771886	3.246515
-37.107560	2.366810	3.256512
-36.611791	3.828388	3.266509
-35.970417	2.607139	3.276506
-35.219599	1.972380	3.286502
-35.001350	0.548729	3.296499
-33.804974	-4.414427	3.306496
-33.816114	7.625072	3.316493
-33.244877	0.361804	3.326490
-32.893686	-2.154183	3.336486
-32.495617	-3.692967	3.346483
-31.946884	-4.694570	3.356480
-31.548958	-0.572895	3.366477
-30.480278	3.006969	3.376474
-30.344665	3.908362	3.386470
-29.870595	-1.085546	3.396467
-29.479191	-4.677328	3.406464
-28.660305	-2.471801	3.416461
-28.287951	-1.516549	3.426458
-27.969138	-2.325368	3.436454
-27.031608	-1.616836	3.446451
-26.492803	1.248774	3.456448
-26.520394	-0.510567	3.466445
-26.098906	-0.386199	3.476442
-25.288381	-7.251633	3.486438
-24.861103	-2.773038	3.496435
-24.333559	-0.436872	3.506432
-23.628794	1.576533	3.516429
-23.667756	-0.557326	3.526426
-22.680302	-6.966787	3.536422
-21.946361	-5.624868	3.546419
-21.912024	1.517048	3.556416
-21.392131	4.579425	3.566413
-20.498804	-1.293220	3.576410
-20.389832	1.580934	3.586406
-20.206422	-0.796226	3.596403
-19.524278	6.071856	3.606400
-18.722255	8.616273	3.616397
-17.996529	3.547892	3.626394
-17.618891	-0.266463	3.636390
-17.611019	4.410016	3.646387
-16.727895	6.985262	3.656384
-16.185647	5.004314	3.666381
-15.746240	4.260883	3.676378
-15.571171	3.007391	3.686374
-14.611909	3.858344	3.696371
-14.234199	5.385512	3.706368
-14.049080	4.590336	3.716365
-12.780451	-0.483969	3.726362
-12.515400	1.795095	3.736358
-12.762773	4.017937	3.746355
-12.018571	5.240596	3.756352
-11.286859	2.029126	3.766349
-11.158987	7.000884	3.776346
-9.615075	7.986596	3.786342
-9.374098	2.900485	3.796339
-9.494139	-1.854954	3.806336
-9.162717	6.450751	3.816333
-8.086254	4.534669	3.826330
-7.856271	-3.095119	3.836326
-7.580306	-1.336524	3.846323
-6.492085	7.431680	3.856320
-6.751730	14.471922	3.866317
-5.928587	18.713666	3.876314
-5.377962	25.538335	3.886310
-4.941889	23.486843	3.896307
-4.434493	41.082185	3.906304
-4.132534	46.993302	3.916301
-3.381215	48.374043	3.926298
-2.958883	52.747174	3.936294
-2.697773	66.462026	3.946291
-2.251649	74.640103	3.956288
-1.968168	92.550191	3.966285
-1.315705	104.812817	3.976282
0.000000	113.780484	3.981286
-0.417967	128.162646	3.986291
-0.112954	122.492902	3.991296
0.174997	126.692722	3.996301
0.011388	138.649168	4.001306
0.365731	136.878680	4.006310
0.128170	131.736466	4.011315
0.039039	137.297784	4.016320
0.471776	132.469439	4.021325
-0.265174	126.035680	4.026330
-0.111425	126.105799	4.031334
-0.136244	133.961929	4.036339
0.341966	134.078172	4.041344
0.489892	125.708259	4.046349
0.208786	122.289479	4.051354
0.076574	115.764270	4.056358
-0.209362	111.034215	4.061363
-0.372183	110.608559	4.066368
0.414546	126.934091	4.071373
0.120232	138.412924	4.076378
0.101137	136.317891	4.081382
0.012122	129.875705	4.086387
0.319271	133.438706	4.091392
0.057548	134.856154	4.096397
0.005088	138.241901	4.101402
0.461572	141.548109	4.106406
0.332798	134.288829	4.111411
0.479036	130.074276	4.116416
0.479595	133.045720	4.121421
0.140510	126.686976	4.126426
0.213477	124.801465	4.131430
0.299505	138.928302	4.136435
0.392282	132.921131	4.141440
0.516097	127.198904	4.146445
0.107609	126.577520	4.151450
0.337968	133.644088	4.156454
0.220063	131.655008	4.161459
0.179218	136.942521	4.166464
0.120555	135.979047	4.171469
0.231354	143.264331	4.176474
0.424475	132.908647	4.181478
0.582795	137.241034	4.186483
0.187450	142.279407	4.191488
0.608937	140.751968	4.196493
0.530527	142.855192	4.201498
0.381262	137.554104	4.206502
0.422002	144.218728	4.211507
0.166182	137.970908	4.216512
0.445326	134.096653	4.221517
0.384038	133.914073	4.226522
0.712277	140.368091	4.231526
0.209274	141.016618	4.236531
0.250548	140.798703	4.241536
0.505048	141.338175	4.246541
0.217083	142.237624	4.251546
0.642588	139.096504	4.256550
0.405346	139.223868	4.261555
0.743337	145.606219	4.266560
0.664000	143.681595	4.271565
0.464268	138.442735	4.276570
0.851835	151.866474	4.281574
0.811053	155.139191	4.286579
0.424682	139.226993	4.291584
0.874836	144.134637	4.296589
0.451033	148.494748	4.301594
0.959707	147.211182	4.306598
0.809166	141.923131	4.311603
0.719035	139.090975	4.316608
0.907561	136.656877	4.321613
0.504180	143.641120	4.326618
0.647966	143.462470	4.331622
1.047005	149.734468	4.336627
0.546624	145.768473	4.341632
1.029189	147.282312	4.346637
0.886318	160.102233	4.351642
1.092343	147.459063	4.356646
0.661402	145.373026	4.361651
0.650843	149.205510	4.366656
0.873386	150.533694	4.371661
0.646254	157.080866	4.376666
1.054226	157.169865	4.381670
1.081012	160.043434	4.386675
1.138254	158.967229	4.391680
1.042993	155.274749	4.396685
0.627160	157.468579	4.401690
0.988017	155.739832	4.406694
1.002110	158.344561	4.411699
1.196282	155.667791	4.416704
1.425836	157.244443	4.421709
0.762119	157.166355	4.426714
0.845903	144.006283	4.431718
1.215569	154.504735	4.436723
0.908245	146.373391	4.441728
1.149759	148.368386	4.446733
1.017180	148.792576	4.451738
1.101533	144.998921	4.456742
0.841634	154.200740	4.461747
0.993947	155.168972	4.466752
1.133553	162.601640	4.471757
0.995397	154.852736	4.476762
1.489860	161.676671	4.481766
1.324516	153.882739	4.486771
1.273717	157.947245	4.491776
1.436350	154.786898	4.496781
1.026953	152.344063	4.501786
1.126816	150.304712	4.506790
1.165906	161.068267	4.511795
1.157605	166.914977	4.516800
1.321197	158.144624	4.521805
1.198047	153.232890	4.526810
1.159921	151.841744	4.531814
1.352485	155.758798	4.536819
0.889928	160.655569	4.541824
0.965904	163.161646	4.546829
0.999964	164.283647	4.551834
1.269434	152.052858	4.556838
1.123874	157.759294	4.561843
1.038132	157.227139	4.566848
1.437860	147.431804	4.571853
1.013775	161.488617	4.576858
1.286283	167.671461	4.581862
1.567934	169.271851	4.586867
1.546785	180.519789	4.591872
1.597920	173.032970	4.596877
0.961225	161.100620	4.601882
1.402326	174.290551	4.606886
1.558462	179.057647	4.611891
1.526138	180.383637	4.616896
1.928097	179.997461	4.621901
1.382889	182.889184	4.626906
1.367559	187.238302	4.631910
1.598981	190.140744	4.636915
1.437081	184.160529	4.641920
1.621112	184.383700	4.646925
1.389967	185.500284	4.651930
1.408289	183.616316	4.656934
1.589160	186.388203	4.661939
1.457299	187.641874	4.666944
1.936041	180.565940	4.671949
1.584891	187.047425	4.676954
1.869453	176.886140	4.681958
1.365402	181.994425	4.686963
1.448059	183.328805	4.691968
1.665279	178.340178	4.696973
1.310960	184.510200	4.701978
1.573406	186.118113	4.706982
1.780617	197.254051	4.711987
1.728312	189.214249	4.716992
1.634018	183.737294	4.721997
1.782344	191.704496	4.727002
1.853301	183.594558	4.732006
1.420398	182.879335	4.737011
1.628913	192.677514	4.742016
1.738117	187.354921	4.747021
1.535478	190.674970	4.752026
2.076964	201.378056	4.757030
1.812574	197.243123	4.762035
1.782015	192.698086	4.767040
1.746100	196.267785	4.772045
1.774584	211.592376	4.777050
2.268206	204.029310	4.782054
2.055694	195.454613	4.787059
2.013938	195.408118	4.792064
1.966857	185.845995	4.797069
1.597270	197.246955	4.802074
2.155792	195.883697	4.807078
2.093531	206.126523	4.812083
1.965706	203.501287	4.817088
2.030696	185.891017	4.822093
1.900390	201.411008	4.827098
1.879016	195.098295	4.832102
1.999056	206.603680	4.837107
2.111495	212.364701	4.842112
2.257263	215.578322	4.847117
2.020474	227.484201	4.852122
2.518835	207.307028	4.857126
1.963573	210.725531	4.862131
1.639341	196.561839	4.867136
2.019394	203.473213	4.872141
2.067229	221.766091	4.877146
2.732649	212.202399	4.882150
2.225392	215.771019	4.887155
2.038887	218.939612	4.892160
2.547085	214.548079	4.897165
2.046247	208.071636	4.902170
2.048759	201.051266	4.907174
2.201765	212.797867	4.912179
2.531894	205.524331	4.917184
2.447849	204.336738	4.922189
1.943488	207.035613	4.927194
1.857606	201.919369	4.932198
1.992797	219.240109	4.937203
2.087924	213.828669	4.942208
2.613415	203.055593	4.947213
2.026218	212.343611	4.952218
2.214215	213.271009	4.957222
2.139880	222.306572	4.962227
2.051111	217.728739	4.967232
2.199152	222.292157	4.972237
2.284036	213.221436	4.977242
2.522175	219.374670	4.982246
2.645137	211.749248	4.987251
2.213587	217.292308	4.992256
2.195735	206.600517	4.997261
2.186577	211.507081	5.002266
2.111567	225.082074	5.007270
2.760987	240.081080	5.012275
2.429502	239.462727	5.017280
2.796293	249.206909	5.022285
2.574260	245.467910	5.027290
2.499649	231.265022	5.032294
2.589126	235.373810	5.037299
2.482993	238.563631	5.042304
2.719676	237.012320	5.047309
2.507139	233.590449	5.052314
2.742290	225.728979	5.057318
2.651729	224.184693	5.062323
2.413690	227.753335	5.067328
2.527947	219.891166	5.072333
2.774125	240.717183	5.077338
2.610975	243.663659	5.082342
2.744556	250.957852	5.087347
2.863171	253.115490	5.092352
2.659612	229.056090	5.097357
2.434577	231.463822	5.102362
2.705803	240.551696	5.107366
2.615699	241.511925	5.112371
2.612938	251.431362	5.117376
2.766010	248.054917	5.122381
2.725713	250.910799	5.127386
2.717477	248.665754	5.132390
2.883526	248.004877	5.137395
2.433966	248.228375	5.142400
3.123958	243.953550	5.147405
2.450912	252.245446	5.152410
2.706783	251.992193	5.157414
2.873267	255.146150	5.162419
2.734874	257.024491	5.167424
3.257054	244.876697	5.172429
2.729977	253.858978	5.177434
2.819676	249.639941	5.182438
2.722546	250.696055	5.187443
2.718795	250.607154	5.192448
2.840364	247.969030	5.197453
2.761553	262.188396	5.202458
2.821806	259.747696	5.207462
3.013612	250.749826	5.212467
2.873450	250.513013	5.217472
3.025628	244.334936	5.222477
2.926194	244.407315	5.227482
2.931058	250.764951	5.232486
2.764838	254.846030	5.237491
3.072661	259.952908	5.242496
3.354533	267.935925	5.247501
3.570577	268.249109	5.252506
3.453787	266.165698	5.257510
3.106412	260.210049	5.262515
3.130746	252.412088	5.267520
3.238614	251.035041	5.272525
3.171078	255.202196	5.277530
2.773679	250.237964	5.282534
2.794531	255.388808	5.287539
3.072675	265.184384	5.292544
3.327490	257.260835	5.297549
3.512567	265.171866	5.302554
3.025220	250.717620	5.307558
2.850616	268.781180	5.312563
3.109697	273.893963	5.317568
3.366408	271.728575	5.322573
3.344773	279.876508	5.327578
3.254593	275.516751	5.332582
3.630418	277.969445	5.337587
3.106964	280.820089	5.342592
3.100956	277.437814	5.347597
3.012608	278.615219	5.352602
3.303938	282.497007	5.357606
3.411320	276.421057	5.362611
3.283853	285.081239	5.367616
3.800534	277.112543	5.372621
3.565125	277.972907	5.377626
3.273480	272.291795	5.382630
3.602600	272.624539	5.387635
3.446818	274.634820	5.392640
3.508596	274.679518	5.397645
3.487495	274.664925	5.402650
3.392002	260.133943	5.407654
3.559541	276.075928	5.412659
3.435444	272.596582	5.417664
3.599277	277.850645	5.422669
3.465349	274.242092	5.427674
3.461663	272.136794	5.432678
3.441658	270.460839	5.437683
2.906755	273.717720	5.442688
3.856805	266.385905	5.447693
3.351989	275.520802	5.452698
3.534610	273.407939	5.457702
3.575074	274.097116	5.462707
3.209201	274.111789	5.467712
3.602920	269.912656	5.472717
3.403292	277.616848	5.477722
3.305891	274.608465	5.482726
3.722766	287.111827	5.487731
3.714906	284.936966	5.492736
4.047704	275.862454	5.497741
3.683551	276.144627	5.502746
3.935813	271.772174	5.507750
3.880037	275.383266	5.512755
3.477232	281.485379	5.517760
3.749086	277.155462	5.522765
3.595107	272.279776	5.527770
3.955318	275.373834	5.532774
3.567139	268.264994	5.537779
3.637665	279.030530	5.542784
3.837747	285.625811	5.547789
4.018002	308.516717	5.552794
4.103361	295.850190	5.557798
3.667791	279.985461	5.562803
3.538759	298.688182	5.567808
3.925244	292.984166	5.572813
3.790502	312.345573	5.577818
3.874239	302.775530	5.582822
4.022572	306.260083	5.587827
3.850100	310.861405	5.592832
3.882648	307.241855	5.597837
3.867270	307.187636	5.602842
4.135507	306.102729	5.607846
4.211666	312.808922	5.612851
3.816136	314.599409	5.617856
4.071179	311.766108	5.622861
3.596791	308.364097	5.627866
4.057285	304.010040	5.632870
4.041042	307.504479	5.637875
4.051423	318.929833	5.642880
4.504736	308.835438	5.647885
4.287682	311.613644	5.652890
4.317783	310.743010	5.657894
4.171935	308.250786	5.662899
4.212173	311.521368	5.667904
3.799270	295.198007	5.672909
3.994396	303.229151	5.677914
4.363119	306.536706	5.682918
4.429402	307.747117	5.687923
4.447855	312.696699	5.692928
4.195286	280.094916	5.697933
3.901745	295.826738	5.702938
4.277409	296.928888	5.707942
4.480983	309.742282	5.712947
4.173814	303.924803	5.717952
4.120447	290.461120	5.722957
4.313627	300.481937	5.727962
4.132780	309.779689	5.732966
4.299682	306.549536	5.737971
3.982730	308.201504	5.742976
4.441965	308.633474	5.747981
4.165609	323.582010	5.752986
4.167959	313.290158	5.757990
4.524258	311.125443	5.762995
4.496290	314.801797	5.768000
4.295391	308.767606	5.773005
3.936156	315.345008	5.778010
4.145899	311.138440	5.783014
4.261694	308.939942	5.788019
4.183733	317.394806	5.793024
4.126296	315.850551	5.798029
4.195477	321.942015	5.803034
4.484753	322.545592	5.808038
4.485612	323.144831	5.813043
4.676528	330.202432	5.818048
4.533784	321.409105	5.823053
4.322284	326.001699	5.828058
4.465093	327.946954	5.833062
4.635614	344.168735	5.838067
4.875992	336.385476	5.843072
4.615742	325.331371	5.848077
4.391593	323.833468	5.853082
4.429636	319.561002	5.858086
4.873568	335.829855	5.863091
4.665579	329.987063	5.868096
4.439474	316.748903	5.873101
4.758522	323.393174	5.878106
4.567134	330.120786	5.883110
4.809142	331.376103	5.888115
4.397798	336.983546	5.893120
4.435152	328.001932	5.898125
4.623527	337.630473	5.903130
4.829316	336.860593	5.908134
4.891101	338.173775	5.913139
4.795437	347.555718	5.918144
4.984560	330.798539	5.923149
4.969989	336.554195	5.928154
4.591635	337.890529	5.933158
5.005118	332.521646	5.938163
4.782020	343.497861	5.943168
4.875714	337.702991	5.948173
4.745488	351.500165	5.953178
4.712247	334.715076	5.958182
5.168975	334.153276	5.963187
4.737775	349.705874	5.968192
4.680664	340.315027	5.973197
4.886343	341.949328	5.978202
4.870334	338.054631	5.983206
4.787752	337.207588	5.988211
5.021329	342.925313	5.993216
4.788503	342.746665	5.998221
4.811218	346.993031	6.003226
4.456816	343.048199	6.008230
4.976177	348.287026	6.013235
5.031928	344.356765	6.018240
4.984767	345.784881	6.023245
4.769729	344.228634	6.028250
4.495737	342.806867	6.033254
4.439310	343.888808	6.038259
4.591368	342.691117	6.043264
5.122816	342.722573	6.048269
4.643192	341.495687	6.053274
4.589643	342.692593	6.058278
4.795738	345.293188	6.063283
4.807281	366.146978	6.068288
5.106417	364.602087	6.073293
4.912200	366.343260	6.078298
5.242442	364.980295	6.083302
5.121839	351.089997	6.088307
4.392163	340.958019	6.093312
4.980873	348.855143	6.098317
4.845054	351.306532	6.103322
4.992859	358.470348	6.108326
5.067721	349.880146	6.113331
4.669427	348.821736	6.118336
4.815564	352.118206	6.123341
4.844715	358.441672	6.128346
5.107865	364.746916	6.133350
5.227631	342.466871	6.138355
4.759963	344.861319	6.143360
4.877196	341.122754	6.148365
4.785181	340.182945	6.153370
5.008366	358.448725	6.158374
5.097024	340.143876	6.163379
4.950743	341.823236	6.168384
4.905755	345.393485	6.173389
4.985284	347.314292	6.178394
4.544332	344.077039	6.183398
5.211131	337.873108	6.188403
5.011722	340.768181	6.193408
5.017653	332.722806	6.198413
5.029781	341.822069	6.203418
4.629990	338.237199	6.208422
4.897348	342.641378	6.213427
4.679463	345.080306	6.218432
4.858366	346.044542	6.223437
4.602410	348.303489	6.228442
4.780790	365.405695	6.233446
5.136404	371.953354	6.238451
4.905554	370.058526	6.243456
5.249388	362.807117	6.248461
5.025896	351.682377	6.253466
4.707507	352.313365	6.258470
5.082770	346.032594	6.263475
4.640713	332.001954	6.268480
5.026446	334.792832	6.273485
4.904820	339.714508	6.278490
4.997485	340.273878	6.283494
4.806835	338.210975	6.288499
4.449527	348.898809	6.293504
4.810303	353.378691	6.298509
4.998545	368.006627	6.303514
5.042058	363.118733	6.308518
5.032003	362.670930	6.313523
5.189466	378.857613	6.318528
4.992174	346.577472	6.323533
4.935528	337.760407	6.328538
5.060025	334.525430	6.333542
4.925334	333.349766	6.338547
4.933699	340.157972	6.343552
4.970580	333.809705	6.348557
4.919780	328.922638	6.353562
4.794740	340.298207	6.358566
4.784787	336.499203	6.363571
4.741261	339.451148	6.368576
4.881307	327.042341	6.373581
4.765150	342.220709	6.378586
5.384795	354.716401	6.383590
5.201798	345.851778	6.388595
4.656486	343.452927	6.393600
4.781356	337.734000	6.398605
4.826632	335.608153	6.403610
4.806903	337.350623	6.408614
4.934966	327.754083	6.413619
5.006434	339.010677	6.418624
5.237056	337.378662	6.423629
5.211320	334.795503	6.428634
5.122130	341.721887	6.433638
5.193537	340.923938	6.438643
4.800951	341.765734	6.443648
4.970853	334.630362	6.448653
4.757812	338.681129	6.453658
4.988353	343.563633	6.458662
4.950505	337.594194	6.463667
4.774279	346.602892	6.468672
5.167916	348.287966	6.473677
4.898595	340.747172	6.478682
4.884518	330.408102	6.483686
4.881147	335.178965	6.488691
4.809877	343.085518	6.493696
4.948956	341.091943	6.498701
4.732581	336.767077	6.503706
4.486253	331.792800	6.508710
4.779644	330.638408	6.513715
4.121615	343.339934	6.518720
4.664745	351.884770	6.523725
5.008677	363.024040	6.528730
5.384056	370.954527	6.533734
5.330566	358.954459	6.538739
5.057596	350.229647	6.543744
5.103048	343.681829	6.548749
5.263534	343.779842	6.553754
5.113418	349.033029	6.558758
5.319599	341.914143	6.563763
5.021086	343.118262	6.568768
4.985135	347.701331	6.573773
4.712687	343.940463	6.578778
4.796755	339.302795	6.583782
4.995354	338.876881	6.588787
4.785810	337.947851	6.593792
4.960677	343.749102	6.598797
4.782510	342.272000	6.603802
4.961476	344.739345	6.608806
5.170510	344.166857	6.613811
4.761035	350.460138	6.618816
4.815155	347.402576	6.623821
4.768458	350.684207	6.628826
4.931088	344.656309	6.633830
4.975750	351.774842	6.638835
4.913649	346.427280	6.643840
4.918448	342.655630	6.648845
5.154964	346.797130	6.653850
5.064936	343.164715	6.658854
5.070096	340.443828	6.663859
4.941508	349.202112	6.668864
5.057633	350.018873	6.673869
4.731078	338.088705	6.678874
4.578520	352.476065	6.683878
5.377048	336.893165	6.688883
4.909486	346.799051	6.693888
4.838439	340.302297	6.698893
5.082033	341.711670	6.703898
5.488438	348.347999	6.708902
5.057514	332.471592	6.713907
4.615381	320.794026	6.718912
4.815441	314.317118	6.723917
4.665089	328.558653	6.728922
4.688310	338.751497	6.733926
5.163065	335.492463	6.738931
4.950250	348.789641	6.743936
4.912091	344.251146	6.748941
4.976869	347.422556	6.753946
5.036714	344.642489	6.758950
4.982612	329.414696	6.763955
4.345348	321.522601	6.768960
4.807378	340.098491	6.773965
4.856077	335.983902	6.778970
4.914611	343.182621	6.783974
5.246283	339.652655	6.788979
4.842609	339.712857	6.793984
4.751410	343.289771	6.798989
5.237380	343.816773	6.803994
5.059307	345.713141	6.808998
4.938062	342.705535	6.814003
4.734638	344.013299	6.819008
4.746210	343.085148	6.824013
4.954884	337.943173	6.829018
4.624306	345.854382	6.834022
4.744884	341.523053	6.839027
4.684211	347.120386	6.844032
5.078998	346.102138	6.849037
5.001284	340.754993	6.854042
5.018561	345.889290	6.859046
5.072622	338.445123	6.864051
4.863924	345.505162	6.869056
4.802685	347.484602	6.874061
4.875821	337.993254	6.879066
4.874014	348.705103	6.884070
5.222760	334.969564	6.889075
4.942468	345.010400	6.894080
5.162533	347.864234	6.899085
5.291351	335.205279	6.904090
4.683739	333.533278	6.909094
4.886814	314.175860	6.914099
4.716142	334.910200	6.919104
4.901578	319.901658	6.924109
4.745759	329.960156	6.929114
4.964035	345.752913	6.934118
5.166691	343.017083	6.939123
4.800153	339.238447	6.944128
4.723430	342.620165	6.949133
5.146178	344.312652	6.954138
4.821103	342.606101	6.959142
4.910180	339.331008	6.964147
4.448143	351.416758	6.969152
4.610636	342.719301	6.974157
5.006068	340.724126	6.979162
4.918911	347.767592	6.984166
4.857188	334.175801	6.989171
4.723846	348.218779	6.994176
5.036812	340.104601	6.999181
4.879695	350.528796	7.004186
4.847316	341.069521	7.009190
4.827655	336.954017	7.014195
4.576382	341.389609	7.019200
4.690321	340.724529	7.024205
4.719753	341.505521	7.029210
4.663369	356.268477	7.034214
4.830488	344.718328	7.039219
4.947582	346.305729	7.044224
4.839573	346.901487	7.049229
4.691812	346.027347	7.054234
4.613701	345.757761	7.059238
4.960019	353.282984	7.064243
4.796695	365.121944	7.069248
5.230965	367.577999	7.074253
5.091410	346.598523	7.079258
4.669431	361.288424	7.084262
5.029638	336.580590	7.089267
4.968439	343.294346	7.094272
4.883372	350.367068	7.099277
4.788242	340.719465	7.104282
4.869313	344.459468	7.109286
4.758238	333.075572	7.114291
4.879974	349.688469	7.119296
5.152832	361.743313	7.124301
4.910251	355.885124	7.129306
4.899445	354.017602	7.134310
4.947773	350.785367	7.139315
4.783429	342.431129	7.144320
4.842151	343.270814	7.149325
5.062891	345.741109	7.154330
4.669896	352.318393	7.159334
5.073171	355.063746	7.164339
4.768190	350.084375	7.169344
4.929514	359.463041	7.174349
5.087226	367.919164	7.179354
4.896936	362.753456	7.184358
5.234341	351.814873	7.189363
4.716160	352.104003	7.194368
4.529289	346.553518	7.199373
5.101918	358.034986	7.204378
5.122539	360.659784	7.209382
5.402011	350.866277	7.214387
4.910132	352.221411	7.219392
4.914742	344.579014	7.224397
5.015188	343.259429	7.229402
4.665144	343.260824	7.234406
4.818826	345.676510	7.239411
4.993089	348.875968	7.244416
4.830167	344.440619	7.249421
5.104541	345.887126	7.254426
5.048061	341.295029	7.259430
4.969783	342.237321	7.264435
5.095117	342.208742	7.269440
4.845275	340.639512	7.274445
5.246921	339.459497	7.279450
4.989684	339.184446	7.284454
5.290050	337.692635	7.289459
4.864737	351.358897	7.294464
5.161344	348.210466	7.299469
5.136155	353.749236	7.304474
5.005361	353.382602	7.309478
5.195669	351.452769	7.314483
5.100594	341.721288	7.319488
4.954289	330.649297	7.324493
4.840807	322.274611	7.329498
4.834380	321.124477	7.334502
5.032743	317.858723	7.339507
4.534884	320.285399	7.344512
4.971819	320.621209	7.349517
4.728083	336.013693	7.354522
4.531777	338.364784	7.359526
5.321363	338.567804	7.364531
5.046354	351.153422	7.369536
5.148515	338.284176	7.374541
5.100089	330.439023	7.379546
4.855568	318.249601	7.384550
4.707878	312.473991	7.389555
4.789824	319.684017	7.394560
4.938727	330.618556	7.399565
4.887648	331.269217	7.404570
4.696250	337.053562	7.409574
4.925209	339.218398	7.414579
5.017571	345.990596	7.419584
4.885616	338.431003	7.424589
5.094286	351.837376	7.429594
4.697604	336.189733	7.434598
5.146180	336.151241	7.439603
4.885127	342.616687	7.444608
4.990293	328.391045	7.449613
4.854979	319.526829	7.454618
4.874656	320.704308	7.459622
4.942641	327.328387	7.464627
4.933378	335.591913	7.469632
4.946656	335.275029	7.474637
5.111150	315.553595	7.479642
4.448885	316.132200	7.484646
4.809915	317.669338	7.489651
5.219625	337.198147	7.494656
4.873833	318.608871	7.499661
5.151737	330.691864	7.504666
4.723534	321.244271	7.509670
4.821294	323.673160	7.514675
5.122068	332.432760	7.519680
4.809789	334.994472	7.524685
4.925865	331.091719	7.529690
4.701217	332.269201	7.534694
5.126373	332.869421	7.539699
4.791442	332.351092	7.544704
4.939327	342.271296	7.549709
5.170190	343.788550	7.554714
4.697991	336.746082	7.559718
4.707292	328.710215	7.564723
4.451733	342.196410	7.569728
4.862058	338.414050	7.574733
4.870085	342.218442	7.579738
4.968112	343.924640	7.584742
4.915977	342.019167	7.589747
4.853422	350.787237	7.594752
5.086816	347.830626	7.599757
5.370828	336.274349	7.604762
5.035857	349.881053	7.609766
4.979210	326.040492	7.614771
4.646325	321.463780	7.619776
4.895638	334.027685	7.624781
5.154477	336.954031	7.629786
4.870014	337.011070	7.634790
4.803617	321.230210	7.639795
5.020077	337.219018	7.644800
4.732728	325.665597	7.649805
4.763331	336.181245	7.654810
4.731352	344.656728	7.659814
5.201873	336.622235	7.664819
4.969958	345.293432	7.669824
5.090561	346.040778	7.674829
4.883015	336.329108	7.679834
5.027809	344.538712	7.684838
4.995966	317.003057	7.689843
4.744129	319.415241	7.694848
4.533214	323.121890	7.699853
4.991030	331.780300	7.704858
4.651417	341.232629	7.709862
5.315789	338.705695	7.714867
4.729511	344.670082	7.719872
4.712043	342.667699	7.724877
4.817002	342.820097	7.729882
4.864244	347.627971	7.734886
4.819809	337.892645	7.739891
4.731164	344.311783	7.744896
5.106753	342.972687	7.749901
5.246234	344.206896	7.754906
4.935969	339.880604	7.759910
5.515448	338.429404	7.764915
5.212045	333.296052	7.769920
4.805443	318.291811	7.774925
4.896799	309.966291	7.779930
4.569225	311.727370	7.784934
4.846931	305.566569	7.789939
4.498888	318.842304	7.794944
4.691456	331.068684	7.799949
5.245024	329.554483	7.804954
4.948918	338.941194	7.809958
5.333337	329.976110	7.814963
4.882984	326.915850	7.819968
4.994886	311.115738	7.824973
4.721304	321.220174	7.829978
4.582623	312.344088	7.834982
5.363096	320.919462	7.839987
4.935312	320.427955	7.844992
4.732213	313.888746	7.849997
4.988931	328.660412	7.855002
5.045021	324.856001	7.860006
4.878347	313.957500	7.865011
4.775235	314.166849	7.870016
4.553996	318.810190	7.875021
5.171943	333.556383	7.880026
5.028304	336.347104	7.885030
5.114764	327.128052	7.890035
4.848850	316.663548	7.895040
4.610236	319.820464	7.900045
5.332806	307.756262	7.905050
5.117281	322.922255	7.910054
5.075332	309.739448	7.915059
5.012604	318.769987	7.920064
4.672843	315.019878	7.925069
4.687428	313.043568	7.930074
4.297893	313.740406	7.935078
4.800450	326.215798	7.940083
5.210749	341.656673	7.945088
5.282050	330.468926	7.950093
5.396568	317.418666	7.955098
5.152329	318.227607	7.960102
5.524285	312.804038	7.965107
5.085197	311.855199	7.970112
5.140696	310.544639	7.975117
5.140223	309.644533	7.980122
5.016789	311.545493	7.985139
4.967238	320.283935	7.990157
5.154834	311.531825	7.995174
5.018241	301.010526	8.000192
4.950106	289.438618	8.005210
4.736261	283.725577	8.010227
4.508030	290.242799	8.015245
5.196023	302.619213	8.020262
4.924538	308.667661	8.025280
5.007472	305.439506	8.030298
4.987586	316.103774	8.035315
5.234760	307.638824	8.040333
4.877389	303.836585	8.045350
4.892827	306.577564	8.050368
5.045672	307.112905	8.055386
5.062236	314.844615	8.060403
4.899087	308.526369	8.065421
4.981594	304.351318	8.070438
4.924304	305.683201	8.075456
4.735695	313.070372	8.080474
4.777906	307.133836	8.085491
4.791181	310.918983	8.090509
4.874816	310.136763	8.095526
4.875356	314.723952	8.100544
4.998878	305.800187	8.105562
4.856391	306.121265	8.110579
4.734927	305.521026	8.115597
5.005293	305.919988	8.120614
5.087745	307.566892	8.125632
5.032907	313.793820	8.130650
4.782860	315.420592	8.135667
4.996753	299.985763	8.140685
5.143628	306.696763	8.145702
4.856044	304.932598	8.150720
5.042094	307.132574	8.155738
4.950555	306.787594	8.160755
4.953595	313.646617	8.165773
5.181346	332.698117	8.170790
5.072177	337.382410	8.175808
5.460402	338.411409	8.180826
5.169404	320.455261	8.185843
5.226919	312.374440	8.190861
4.976571	307.441975	8.195878
4.569341	314.773820	8.200896
5.228889	320.823605	8.205914
5.118389	331.031668	8.210931
5.400365	340.307497	8.215949
5.210395	335.407148	8.220966
5.560294	339.660730	8.225984
5.320155	315.433695	8.231002
5.127161	315.435211	8.236019
5.060082	311.509515	8.241037
4.982959	311.643603	8.246054
4.924179	311.726627	8.251072
5.202506	321.428210	8.256090
5.304363	345.010233	8.261107
5.454745	333.015920	8.266125
5.223953	315.353327	8.271142
5.054527	308.660956	8.276160
5.239055	309.659909	8.281178
5.246912	318.784873	8.286195
5.029283	322.631287	8.291213
5.300487	320.167753	8.296230
5.422505	329.465339	8.301248
5.140644	311.377188	8.306266
4.911697	318.022286	8.311283
5.550893	329.082896	8.316301
5.488194	327.130912	8.321318
5.223000	329.387307	8.326336
5.496220	311.114533	8.331354
5.143428	310.575825	8.336371
5.323121	307.741258	8.341389
5.011520	301.869018	8.346406
5.179765	306.493587	8.351424
5.349590	319.247326	8.356442
5.585399	325.453098	8.361459
5.068041	321.397253	8.366477
5.040666	319.813405	8.371494
5.384819	330.540030	8.376512
5.612276	332.180444	8.381530
5.506351	318.557857	8.386547
5.195488	319.221553	8.391565
5.241003	310.827785	8.396582
4.956363	327.879853	8.401600
5.750715	324.829733	8.406618
5.865719	333.277767	8.411635
5.315591	327.215112	8.416653
5.125023	321.626932	8.421670
4.794569	316.262097	8.426688
5.455991	323.300662	8.431706
5.465573	332.362755	8.436723
5.327078	339.389898	8.441741
5.582293	343.296395	8.446758
5.360439	340.150392	8.451776
5.398186	336.513408	8.456794
5.626693	343.259525	8.461811
5.443165	344.223371	8.466829
5.126945	331.001903	8.471846
5.251235	340.364074	8.476864
5.638058	332.038571	8.481882
5.478705	339.739191	8.486899
5.580949	338.820042	8.491917
5.436026	336.455723	8.496934
5.098654	344.441117	8.501952
5.585358	330.181652	8.506970
5.422762	340.245211	8.511987
5.570025	336.165915	8.517005
5.609842	333.855448	8.522022
5.662216	346.000167	8.527040
5.615755	335.389123	8.532058
5.395834	332.503016	8.537075
4.906881	330.688734	8.542093
5.600563	326.794922	8.547110
5.356164	342.820744	8.552128
5.487595	330.523494	8.557146
5.629080	335.517432	8.562163
5.353585	339.031138	8.567181
5.680364	326.659618	8.572199
5.624847	342.841943	8.577216
5.471837	330.090062	8.582234
5.539150	335.224618	8.587251
5.498241	332.781861	8.592269
5.553275	330.056311	8.597287
5.191976	348.146797	8.602304
5.431878	335.395791	8.607322
5.482059	338.427454	8.612339
5.485866	326.905018	8.617357
5.827966	327.350955	8.622375
5.470045	341.918335	8.627392
5.312454	337.382278	8.632410
5.583516	338.961146	8.637427
5.301522	336.379583	8.642445
5.736982	337.904262	8.647463
5.613095	335.551813	8.652480
5.459315	339.273299	8.657498
5.282976	335.401906	8.662515
5.401506	343.927308	8.667533
5.591615	355.920301	8.672551
5.853717	370.756663	8.677568
5.950176	358.835033	8.682586
6.027065	348.184856	8.687603
5.280140	346.305030	8.692621
5.566226	342.339546	8.697639
5.679659	346.470488	8.702656
5.603697	339.423482	8.707674
5.605029	356.840005	8.712691
5.625762	366.545692	8.717709
5.852363	374.905590	8.722727
5.962489	372.886600	8.727744
5.758277	349.706233	8.732762
5.497722	343.338360	8.737779
5.470560	349.084185	8.742797
5.785382	367.583362	8.747815
5.836640	375.041662	8.752832
6.128536	362.273954	8.757850
5.688764	351.625869	8.762867
5.543846	344.470407	8.767885
5.984364	341.839868	8.772903
5.575112	354.782627	8.777920
5.547487	351.344639	8.782938
5.959159	366.592414	8.787955
5.686588	377.472765	8.792973
5.914326	365.616393	8.797991
5.679570	376.916234	8.803008
5.756104	370.629923	8.808026
6.174936	367.696499	8.813043
5.521082	359.679908	8.818061
5.715065	352.731098	8.823079
5.811873	361.962805	8.828096
5.781771	363.871049	8.833114
5.660714	367.755219	8.838131
5.634589	363.319816	8.843149
5.966996	366.016980	8.848167
5.584914	366.172041	8.853184
5.904533	364.967703	8.858202
5.770182	372.093379	8.863219
5.636853	374.481869	8.868237
6.074837	370.908908	8.873255
6.026312	372.033456	8.878272
6.052883	368.110938	8.883290
5.857817	367.741370	8.888307
5.674180	364.724062	8.893325
5.820931	364.608893	8.898343
5.736709	372.310079	8.903360
5.813935	371.034076	8.908378
6.282613	365.596932	8.913395
6.148493	371.733083	8.918413
6.239053	362.691723	8.923431
5.844253	361.388378	8.928448
5.650967	360.556349	8.933466
5.867271	371.443729	8.938483
6.020501	372.671669	8.943501
6.441718	360.385461	8.948519
6.301162	368.301665	8.953536
6.258415	366.730987	8.958554
6.288870	373.184741	8.963571
5.995322	367.380348	8.968589
5.721385	355.140557	8.973607
5.550325	367.824022	8.978624
5.797448	362.945964	8.983642
6.186226	365.052935	8.988659
5.890997	376.783228	8.993677
6.115339	359.867792	8.998695
6.153841	365.926345	9.003712
5.648370	366.816543	9.008730
5.777117	365.281636	9.013747
5.680458	373.969645	9.018765
5.751694	368.058591	9.023783
5.998015	374.918692	9.028800
5.802577	363.316237	9.033818
5.859253	376.914481	9.038835
5.902115	384.339926	9.043853
6.191999	393.114714	9.048871
6.264377	397.909306	9.053888
6.258838	395.445526	9.058906
6.305341	379.178365	9.063923
5.664966	380.711915	9.068941
6.002443	386.250339	9.073959
6.293348	386.144367	9.078976
6.374577	396.660659	9.083994
6.328853	376.641945	9.089011
5.928251	383.172395	9.094029
5.939783	375.252096	9.099047
6.082790	379.214580	9.104064
6.245814	377.721826	9.109082
6.194838	377.458704	9.114099
5.961989	401.811139	9.119117
6.255012	390.524995	9.124135
6.251205	405.844560	9.129152
6.116239	397.639279	9.134170
6.361984	393.256086	9.139187
6.200047	401.680926	9.144205
6.143422	396.904135	9.149223
6.470453	403.284385	9.154240
6.473154	404.278809	9.159258
6.321524	376.361525	9.164275
5.919591	381.082301	9.169293
6.437175	385.088069	9.174311
6.388126	385.094487	9.179328
6.433121	380.997865	9.184346
6.188423	363.037544	9.189363
5.854411	379.641583	9.194381
6.062318	392.729995	9.199399
6.613799	390.975097	9.204416
6.371021	400.079017	9.209434
6.234971	400.531107	9.214451
6.297047	397.977790	9.219469
6.575087	401.420519	9.224487
6.420309	399.317644	9.229504
5.905381	401.461477	9.234522
6.504055	393.250456	9.239539
6.037971	401.424305	9.244557
6.448641	398.421957	9.249575
6.850231	399.930206	9.254592
6.272550	396.710051	9.259610
6.292431	391.443662	9.264627
6.316430	392.373934	9.269645
6.295786	400.998391	9.274663
6.676463	405.177019	9.279680
6.297745	411.393055	9.284698
6.511787	406.895629	9.289715
6.225000	405.514557	9.294733
6.268365	399.742938	9.299751
6.380066	397.889222	9.304768
6.339004	401.735550	9.309786
6.485225	401.148655	9.314803
6.180573	407.066227	9.319821
6.270950	408.186280	9.324839
6.492992	405.598600	9.329856
6.298062	411.400572	9.334874
6.648283	402.414413	9.339891
6.166920	408.227399	9.344909
6.619697	399.461051	9.349927
6.354189	394.218495	9.354944
6.795771	412.937860	9.359962
6.861061	402.643475	9.364979
6.424039	412.697802	9.369997
6.578787	400.466512	9.375015
6.828216	395.286314	9.380032
6.359662	393.489118	9.385050
6.473144	399.778753	9.390067
6.713056	406.465336	9.395085
6.338187	401.748327	9.400103
6.272184	400.656262	9.405120
6.120781	404.600382	9.410138
6.468527	405.423901	9.415155
6.275077	408.026076	9.420173
6.057516	404.432927	9.425191
6.392669	401.057484	9.430208
6.325451	409.141276	9.435226
6.593748	420.970794	9.440243
6.763812	431.449763	9.445261
6.456817	427.524594	9.450279
6.568054	419.040757	9.455296
6.621889	432.798563	9.460314
6.797188	439.811977	9.465331
6.989311	428.348827	9.470349
6.588052	421.523745	9.475367
6.779371	403.944883	9.480384
6.409429	402.284101	9.485402
6.470094	408.563392	9.490419
6.458045	417.558454	9.495437
6.995465	429.456792	9.500455
7.144486	419.207779	9.505472
6.656693	413.715235	9.510490
6.578431	402.500993	9.515507
6.715793	405.770970	9.520525
6.379870	412.194274	9.525543
6.734669	416.680119	9.530560
6.578490	426.266330	9.535578
6.910331	428.229797	9.540595
6.902721	432.410921	9.545613
6.621399	436.141935	9.550631
6.825543	428.466071	9.555648
6.984949	433.731856	9.560666
6.764437	421.852822	9.565683
6.300534	419.386597	9.570701
6.391028	427.981644	9.575719
6.944129	425.050581	9.580736
6.596785	437.617832	9.585754
6.705547	437.984506	9.590771
6.696921	431.588856	9.595789
6.507644	438.072526	9.600807
6.635965	434.951977	9.605824
6.866179	439.114784	9.610842
6.483014	431.341106	9.615859
6.713199	431.721727	9.620877
6.588410	434.561729	9.625895
7.059576	425.357907	9.630912
7.011432	438.660791	9.635930
6.758329	427.376081	9.640947
6.874468	431.233390	9.645965
6.859006	431.049419	9.650983
6.962485	432.726710	9.656000
6.721960	438.735440	9.661018
6.635291	434.517506	9.666035
6.956741	449.355926	9.671053
6.947749	454.355727	9.676071
7.149372	437.427631	9.681088
6.943692	444.529721	9.686106
7.010183	437.517936	9.691123
6.888062	429.938219	9.696141
6.768152	431.126163	9.701159
7.115716	437.646126	9.706176
6.894141	437.264019	9.711194
7.039925	429.367717	9.716211
7.080518	430.028335	9.721229
6.813563	439.730921	9.726247
7.061712	428.198656	9.731264
7.104141	422.570283	9.736282
7.025771	439.259012	9.741299
6.945752	436.764648	9.746317
6.775088	436.729005	9.751335
7.332250	448.372139	9.756352
6.994921	450.547983	9.761370
7.102866	433.978093	9.766387
7.182294	447.541531	9.771405
6.944114	439.794624	9.776423
7.195865	433.965653	9.781440
6.704517	438.961666	9.786458
6.906142	447.219841	9.791475
7.405670	460.093302	9.796493
7.319902	460.250869	9.801511
7.504205	445.968739	9.806528
7.094045	443.381415	9.811546
7.095336	436.946722	9.816563
7.106410	430.993838	9.821581
6.947605	435.311605	9.826599
7.418025	429.471228	9.831616
7.039068	435.409579	9.836634
7.142390	429.988820	9.841651
7.328069	429.247370	9.846669
7.620070	445.021890	9.851687
7.517554	435.797120	9.856704
7.351425	440.688301	9.861722
7.042616	431.219171	9.866739
7.397967	440.610067	9.871757
7.058452	444.501888	9.876775
7.076802	437.091413	9.881792
6.915927	437.211616	9.886810
7.317470	436.881041	9.891827
7.330445	434.106339	9.896845
6.981726	441.421468	9.901863
7.146165	432.365472	9.906880
6.953615	438.386334	9.911898
6.992795	440.549434	9.916915
7.158630	438.943225	9.921933
7.188517	460.608159	9.926951
7.681628	465.349047	9.931968
7.262969	462.244859	9.936986
7.066292	448.372440	9.942003
7.395492	455.933169	9.947021
7.411685	453.703952	9.952039
7.420983	463.198223	9.957056
7.370104	460.554947	9.962074
7.343286	460.038825	9.967091
7.523425	446.008351	9.972109
7.168401	445.337734	9.977127
7.565638	445.154317	9.982144
7.163549	441.499990	9.987162
7.594865	453.774157	9.992179
7.605565	442.648297	9.997197
7.467859	431.578514	10.002215
7.141336	435.874450	10.007232
7.208124	437.341889	10.012250
7.352635	446.361826	10.017267
7.462999	448.767254	10.022285
7.571529	460.648059	10.027303
7.732844	447.077556	10.032320
7.493083	437.897360	10.037338
7.146834	444.020637	10.042355
7.039652	437.402346	10.047373
7.488734	444.760162	10.052391
7.703858	457.439000	10.057408
7.804302	461.482564	10.062426
7.426113	455.094756	10.067443
7.411770	438.866542	10.072461
7.309428	457.758699	10.077479
7.414822	457.809224	10.082496
7.652834	461.319023	10.087514
7.308675	461.724085	10.092531
7.283579	464.019278	10.097549
7.452875	458.127580	10.102567
7.632093	450.911900	10.107584
7.787625	461.092138	10.112602
7.347472	471.741268	10.117619
7.929706	461.343923	10.122637
7.726906	468.545146	10.127655
7.367765	467.097316	10.132672
7.274860	457.340272	10.137690
7.260116	470.098519	10.142707
7.276809	455.951804	10.147725
7.278407	469.459847	10.152743
7.640462	462.954776	10.157760
7.101732	467.675004	10.162778
7.296962	461.071386	10.167795
7.754764	473.712415	10.172813
7.792461	489.921187	10.177831
7.527355	484.703925	10.182848
7.896151	487.118137	10.187866
7.551851	480.720180	10.192883
7.692355	480.507233	10.197901
7.166540	495.951314	10.202919
7.627274	500.004514	10.207936
7.613641	503.427262	10.212954
7.719076	494.805574	10.217971
7.979094	495.586543	10.222989
7.573867	510.076289	10.228007
7.272116	499.797345	10.233024
7.753271	496.506556	10.238042
7.759426	491.310905	10.243059
7.885006	498.721527	10.248077
7.839868	496.308379	10.253095
7.900816	495.144896	10.258112
7.796408	493.250975	10.263130
7.744771	500.366950	10.268147
8.142356	489.453942	10.273165
7.248343	501.562987	10.278183
7.499282	497.921764	10.283200
7.500557	492.785381	10.288218
7.251521	500.528685	10.293235
7.902714	502.991407	10.298253
7.935100	519.593974	10.303271
7.988693	514.906762	10.308288
7.653313	515.083222	10.313306
7.425810	516.028181	10.318323
8.317248	518.952466	10.323341
8.213544	523.964036	10.328359
8.000165	518.175442	10.333376
7.866746	500.291213	10.338394
8.029361	502.926169	10.343411
8.057259	493.486083	10.348429
8.045276	502.060347	10.353447
8.014327	484.526072	10.358464
7.957386	488.836631	10.363482
7.819937	501.291230	10.368499
7.992452	485.738471	10.373517
8.003165	494.682764	10.378535
7.860202	493.808932	10.383552
8.088389	492.754754	10.388570
8.189620	501.344914	10.393587
8.161739	492.873247	10.398605
7.939610	500.344005	10.403623
7.942322	488.247655	10.408640
7.945239	501.032922	10.413658
7.540779	504.475310	10.418675
8.181553	504.230702	10.423693
8.464574	519.902856	10.428711
8.235737	512.025240	10.433728
7.926526	502.525230	10.438746
8.022587	498.223482	10.443763
8.090771	496.937943	10.448781
7.956966	494.942597	10.453799
7.981015	492.928200	10.458816
8.302949	499.702219	10.463834
7.881867	494.846583	10.468851
8.409373	504.236175	10.473869
8.248285	506.909183	10.478887
8.190006	489.010753	10.483904
8.362009	487.308841	10.488922
7.900999	492.569512	10.493939
8.082559	493.605580	10.498957
7.981493	491.749883	10.503975
8.110163	511.698851	10.508992
8.466824	512.412247	10.514010
8.329396	518.456884	10.519027
8.020309	491.549450	10.524045
8.383151	496.927819	10.529063
8.165228	498.981346	10.534080
8.642882	512.796593	10.539098
8.095129	505.035959	10.544115
8.251596	490.841266	10.549133
8.075830	495.344521	10.554151
8.220222	497.849826	10.559168
8.346875	496.302656	10.564186
8.225865	511.272074	10.569203
8.446412	509.678254	10.574221
8.258844	508.786219	10.579239
8.434313	516.818858	10.584256
8.554507	506.245057	10.589274
8.188790	504.555022	10.594291
8.593433	490.920963	10.599309
8.078763	492.664400	10.604327
8.334747	504.339733	10.609344
8.398626	506.069846	10.614362
8.153603	515.702120	10.619379
8.610032	513.207885	10.624397
8.508811	518.920960	10.629415
8.461719	506.394883	10.634432
8.339221	497.790269	10.639450
7.824721	506.292245	10.644467
7.906229	516.067680	10.649485
8.434339	521.034073	10.654503
8.506148	512.661431	10.659520
8.377096	509.523646	10.664538
8.057121	515.693976	10.669555
8.102609	521.693366	10.674573
8.438785	525.382778	10.679591
8.309162	519.603344	10.684608
8.504021	509.736023	10.689626
8.513611	512.409902	10.694643
8.554934	518.660160	10.699661
8.724752	512.616791	10.704679
8.494946	524.064728	10.709696
8.639936	520.561901	10.714714
8.727262	524.392904	10.719731
8.507563	517.019643	10.724749
8.549049	520.790525	10.729767
8.370789	519.189518	10.734784
8.380528	520.999459	10.739802
8.467883	517.770724	10.744819
8.555035	527.605661	10.749837
8.674571	529.826328	10.754855
8.582823	522.780475	10.759872
9.161721	508.514439	10.764890
8.396233	521.347438	10.769907
8.599746	522.923142	10.774925
8.845106	529.012462	10.779943
8.363076	520.522090	10.784960
8.950295	521.389027	10.789978
8.490347	523.762337	10.794995
8.805516	523.250998	10.800013
8.952236	521.273563	10.805031
8.536610	525.686239	10.810048
8.723466	526.033293	10.815066
8.963776	521.280911	10.820083
8.468383	524.744659	10.825101
8.907063	524.273691	10.830119
8.328365	522.900790	10.835136
8.678433	514.153748	10.840154
8.864736	532.876359	10.845171
8.664377	534.145344	10.850189
8.677820	537.040226	10.855207
8.702101	550.616823	10.860224
9.261441	542.389011	10.865242
9.092970	543.809792	10.870259
8.696695	526.237741	10.875277
8.921068	517.253261	10.880295
8.435477	521.809401	10.885312
9.030357	531.796078	10.890330
9.150930	531.808068	10.895347
8.991783	529.944071	10.900365
8.871665	528.257063	10.905383
8.610488	530.157924	10.910400
8.981117	524.696216	10.915418
8.431935	528.027346	10.920435
8.903649	541.916433	10.925453
9.349248	543.397922	10.930471
8.855850	529.169475	10.935488
9.115846	526.796341	10.940506
9.123956	518.639149	10.945523
8.655577	517.522962	10.950541
9.066246	528.881580	10.955559
8.859296	529.295023	10.960576
8.947113	534.294566	10.965594
9.279182	543.573049	10.970611
9.246306	530.232844	10.975629
9.254713	514.610977	10.980647
8.685665	523.487323	10.985664
9.056028	513.964928	10.990682
9.172855	516.783440	10.995699
8.897572	515.185311	11.000717
9.061607	501.959561	11.005735
9.000183	518.800283	11.010752
8.929540	517.404669	11.015770
8.995870	521.798164	11.020787
9.097126	532.583654	11.025805
9.423948	534.825309	11.030823
8.927549	529.289663	11.035840
9.068081	522.658071	11.040858
8.910408	530.996060	11.045875
9.176352	536.191683	11.050893
9.182201	533.692337	11.055911
9.132713	549.667791	11.060928
9.440427	542.914813	11.065946
9.527550	539.719968	11.070963
9.531476	526.104597	11.075981
9.478481	509.127645	11.080999
8.909333	517.518606	11.086016
9.161702	517.134783	11.091034
8.711796	510.351180	11.096051
8.978269	516.019706	11.101069
9.512168	525.613946	11.106087
9.113750	542.535691	11.111104
9.125627	542.701300	11.116122
9.562969	547.766584	11.121139
9.385608	539.698948	11.126157
9.597142	517.005748	11.131175
9.478663	517.934425	11.136192
9.024440	508.124195	11.141210
8.877928	521.554650	11.146227
9.399332	531.903468	11.151245
9.738225	532.438521	11.156263
8.995546	518.681251	11.161280
9.598694	527.622536	11.166298
9.505013	524.141710	11.171315
9.015071	520.302122	11.176333
9.570032	521.898759	11.181351
9.388854	536.832499	11.186368
9.175738	529.369171	11.191386
9.223491	538.950618	11.196403
9.030805	540.391943	11.201421
9.594836	542.914377	11.206439
9.238198	548.191444	11.211456
9.522524	548.176319	11.216474
9.606324	552.249038	11.221491
9.115909	559.647131	11.226509
9.217142	549.740764	11.231527
9.224033	553.953179	11.236544
9.643618	554.036712	11.241562
9.479395	559.861999	11.246579
9.354059	558.108140	11.251597
9.909921	553.239329	11.256615
9.571989	551.856083	11.261632
9.471908	544.042558	11.266650
9.582236	547.142448	11.271667
9.353976	547.317114	11.276685
9.676411	545.045835	11.281703
9.371926	554.847024	11.286720
9.701488	548.155382	11.291738
9.592038	549.754173	11.296755
9.380368	551.897018	11.301773
9.278296	543.911591	11.306791
9.431457	551.306845	11.311808
9.517687	555.843108	11.316826
9.933879	567.445704	11.321843
9.547542	558.089720	11.326861
9.755236	560.347759	11.331879
9.284742	566.897733	11.336896
9.598453	564.452120	11.341914
10.019579	572.724210	11.346931
9.553489	577.385004	11.351949
10.072938	568.376632	11.356967
9.902724	564.786235	11.361984
9.992803	552.647614	11.367002
10.017610	545.978289	11.372019
10.038171	539.043940	11.377037
9.461304	539.356050	11.382055
9.964888	542.269175	11.387072
9.732955	535.892152	11.392090
9.886996	531.433167	11.397107
9.633338	536.606569	11.402125
9.943956	532.151379	11.407143
9.681307	538.512998	11.412160
9.558760	545.925559	11.417178
9.576127	539.048428	11.422195
10.033803	555.716036	11.427213
10.239440	553.119829	11.432231
9.913067	547.614482	11.437248
9.868256	538.326950	11.442266
9.880341	546.467952	11.447283
9.583951	540.496455	11.452301
9.906330	539.585918	11.457319
10.178918	545.239664	11.462336
9.739639	536.700868	11.467354
10.015214	538.465611	11.472371
10.103409	553.417947	11.477389
10.178726	547.384898	11.482407
9.680164	549.267790	11.487424
9.443575	547.394568	11.492442
10.224445	551.089872	11.497459
10.031778	572.271378	11.502477
9.937169	571.152937	11.507495
10.281835	569.000209	11.512512
10.167129	575.692047	11.517530
10.108139	568.756291	11.522547
10.064633	569.290299	11.527565
10.107999	569.576670	11.532583
10.385608	559.970203	11.537600
9.906125	550.802667	11.542618
10.160846	544.944425	11.547635
9.631401	555.355069	11.552653
10.083302	570.888098	11.557671
10.260893	564.229880	11.562688
10.048500	570.973715	11.567706
10.045944	566.222168	11.572723
9.959122	571.801195	11.577741
10.376426	573.429292	11.582759
9.928911	571.945497	11.587776
9.938981	568.791159	11.592794
10.303867	571.396571	11.597811
10.031574	576.425051	11.602829
9.950104	572.938649	11.607847
10.049471	575.745497	11.612864
10.255770	574.376850	11.617882
10.179386	570.837248	11.622899
9.976325	579.067826	11.627917
10.254057	569.913074	11.632935
10.314449	574.695336	11.637952
9.965198	575.473265	11.642970
10.322710	583.832071	11.647987
10.596318	594.638864	11.653005
10.469823	581.564297	11.658023
10.215924	569.246614	11.663040
9.886644	577.711463	11.668058
10.386843	585.754733	11.673075
10.363029	605.240325	11.678093
10.549457	607.514884	11.683111
10.752638	599.392667	11.688128
10.324319	590.824862	11.693146
10.598317	574.892832	11.698163
10.351224	584.468606	11.703181
10.387343	566.397774	11.708199
10.349090	567.583230	11.713216
10.412150	590.005988	11.718234
10.715797	588.461388	11.723251
10.655409	586.513516	11.728269
10.487290	575.282534	11.733287
10.235354	579.122488	11.738304
10.338779	586.303766	11.743322
10.673033	590.043114	11.748339
10.317789	604.684110	11.753357
10.443074	599.471846	11.758375
10.869642	605.561307	11.763392
10.515691	608.037149	11.768410
10.622814	596.223800	11.773427
10.524669	602.376328	11.778445
10.116125	596.054508	11.783463
10.686837	601.852006	11.788480
10.622896	600.823361	11.793498
10.844008	589.766681	11.798515
10.829557	603.994577	11.803533
10.789332	596.367952	11.808551
10.587841	599.986974	11.813568
10.469227	597.611959	11.818586
10.853304	601.755238	11.823603
10.944586	602.144495	11.828621
10.763768	585.919679	11.833639
10.785853	576.358465	11.838656
10.378048	572.105093	11.843674
10.591543	578.966193	11.848691
10.577637	593.325870	11.853709
10.725563	597.493882	11.858727
10.816043	595.591101	11.863744
10.835270	600.883894	11.868762
10.758330	597.547515	11.873779
10.475003	598.566874	11.878797
10.577369	600.018989	11.883815
11.016782	598.125945	11.888832
10.269549	609.753514	11.893850
10.631322	597.626756	11.898867
10.741464	595.588051	11.903885
10.855135	603.509519	11.908903
10.742981	600.275617	11.913920
10.791794	598.685227	11.918938
10.609416	590.244797	11.923955
10.884375	600.600023	11.928973
10.865268	613.591970	11.933991
11.311460	617.371841	11.939008
10.923402	610.300607	11.944026
11.085869	594.032915	11.949043
11.090980	593.607952	11.954061
10.740221	598.263040	11.959079
11.092681	600.885277	11.964096
10.894185	602.835804	11.969114
11.209800	591.769773	11.974131
10.876890	599.674446	11.979149
10.909450	598.475500	11.984167
11.201098	597.893256	11.989184
11.044313	610.943231	11.994202
10.997050	608.558959	11.999219
10.965103	608.161391	12.004237
11.352599	610.633546	12.009255
11.427297	610.639748	12.014272
10.929800	608.671542	12.019290
11.080617	597.939468	12.024307
11.017641	589.388131	12.029325
11.187664	603.126259	12.034343
11.207371	606.414973	12.039360
11.035987	615.118247	12.044378
11.252517	613.556576	12.049395
11.758626	624.449686	12.054413
11.199906	613.520938	12.059431
11.206178	590.927953	12.064448
11.274775	595.715162	12.069466
11.196016	591.945846	12.074483
10.930918	594.043808	12.079501
10.969926	597.744061	12.084519
11.456286	604.439525	12.089536
11.335038	620.403708	12.094554
11.379441	619.119341	12.099571
11.332873	605.797872	12.104589
11.219746	599.891275	12.109607
11.406507	600.704654	12.114624
11.479497	609.678265	12.119642
11.251660	606.976082	12.124659
11.272607	601.371082	12.129677
11.267949	612.241090	12.134695
11.673848	612.658560	12.139712
11.097188	619.346600	12.144730
11.373134	618.640388	12.149747
11.688712	614.646331	12.154765
11.417563	621.446371	12.159783
11.133615	611.287231	12.164800
11.282186	620.538275	12.169818
11.352668	619.599173	12.174835
11.234144	608.478058	12.179853
11.245985	617.308463	12.184871
11.426505	607.808589	12.189888
11.464695	612.428605	12.194906
11.424692	614.670584	12.199923
11.334118	615.728889	12.204941
10.922954	614.967567	12.209959
11.704217	616.165348	12.214976
11.090983	617.362163	12.219994
11.464652	633.769374	12.225011
11.796542	644.919679	12.230029
11.562545	648.680700	12.235047
11.833435	636.185520	12.240064
11.700188	637.167827	12.245082
11.346387	633.037377	12.250099
11.531523	639.820528	12.255117
11.599093	651.903526	12.260135
11.771216	648.111550	12.265152
11.830532	649.103702	12.270170
11.754959	650.391794	12.275187
12.102235	648.117175	12.280205
11.469001	635.289846	12.285223
11.739930	639.636505	12.290240
11.796134	641.835394	12.295258
11.694147	644.241962	12.300275
11.709239	640.174435	12.305293
11.776816	651.927531	12.310311
11.883711	635.039706	12.315328
11.746500	651.275248	12.320346
12.002240	647.704057	12.325363
11.910358	641.496111	12.330381
11.978485	648.589173	12.335399
12.109685	626.763393	12.340416
11.681898	624.719472	12.345434
11.214235	627.929060	12.350451
11.792332	638.169357	12.355469
11.828459	647.509701	12.360487
12.131347	640.423840	12.365504
11.713842	650.223528	12.370522
11.710762	646.903843	12.375539
11.812969	648.598690	12.380557
11.997368	657.457038	12.385575
11.959236	643.151327	12.390592
11.824088	647.969534	12.395610
11.528813	645.086397	12.400627
11.959075	645.262842	12.405645
11.732485	644.496937	12.410663
12.067938	643.553720	12.415680
11.885220	650.933187	12.420698
11.914083	651.829600	12.425715
12.385163	663.504474	12.430733
12.348125	652.324365	12.435751
12.105382	643.825008	12.440768
11.898369	650.068018	12.445786
11.809255	649.870257	12.450803
12.212461	650.226368	12.455821
12.115188	672.594304	12.460839
12.428409	663.563140	12.465856
12.271464	655.170429	12.470874
11.948681	652.192245	12.475891
12.183638	652.049477	12.480909
11.896385	663.476715	12.485927
12.360579	664.858884	12.490944
12.044359	670.749143	12.495962
12.325030	673.409656	12.500979
12.638484	673.593633	12.505997
12.476769	678.804413	12.511015
12.374355	653.476943	12.516032
12.513024	644.569176	12.521050
12.219377	644.639126	12.526067
12.394615	640.273050	12.531085
11.936307	648.757531	12.536103
12.092093	648.991236	12.541120
12.487528	655.382507	12.546138
12.289660	675.510553	12.551155
12.599537	668.678624	12.556173
12.216928	679.176053	12.561191
12.283828	667.720076	12.566208
12.301341	674.334160	12.571226
12.225319	670.881675	12.576243
12.354701	674.769134	12.581261
12.293447	677.001650	12.586279
12.499125	672.752958	12.591296
12.509443	673.686693	12.596314
12.436466	670.083713	12.601331
12.530246	671.791768	12.606349
12.521023	668.213269	12.611367
12.563800	672.581575	12.616384
12.750400	671.409083	12.621402
12.617705	672.828281	12.626419
13.002407	666.146946	12.631437
12.786552	668.883771	12.636455
12.727024	672.965493	12.641472
12.649925	669.550585	12.646490
12.493500	673.123975	12.651507
12.775631	669.108672	12.656525
12.508107	678.067059	12.661543
12.682206	668.729814	12.666560
12.750488	673.357267	12.671578
12.521429	668.359747	12.676595
13.183182	663.142286	12.681613
12.751338	665.965660	12.686631
12.455558	668.948382	12.691648
12.700630	668.466952	12.696666
12.476054	672.620489	12.701683
12.799494	665.328076	12.706701
12.476130	674.389795	12.711719
12.773594	663.405454	12.716736
12.544894	664.878342	12.721754
12.733464	671.562520	12.726771
12.340642	665.008357	12.731789
12.166195	675.800034	12.736807
12.462279	684.761944	12.741824
12.960808	678.446770	12.746842
13.089815	689.601964	12.751859
13.221563	688.630274	12.756877
12.737292	677.456489	12.761895
12.997322	690.347361	12.766912
13.396255	686.657181	12.771930
12.688225	679.050942	12.776947
12.845315	662.960238	12.781965
12.955593	678.894214	12.786983
13.139157	675.307411	12.792000
12.649659	675.880235	12.797018
12.869418	689.837946	12.802035
12.977611	697.451924	12.807053
13.054697	700.218983	12.812071
12.994946	703.681496	12.817088
13.215764	691.162675	12.822106
13.185446	699.136971	12.827123
13.259968	693.353391	12.832141
13.367851	697.610930	12.837159
12.982072	681.658126	12.842176
13.413923	677.838883	12.847194
12.906162	685.992617	12.852211
13.147765	678.014185	12.857229
13.258266	699.987542	12.862247
13.098982	692.904962	12.867264
13.245625	688.498729	12.872282
13.228580	702.191744	12.877299
13.500897	689.451024	12.882317
13.021509	686.184611	12.887335
12.959026	683.582191	12.892352
13.109945	688.640033	12.897370
12.867602	691.332432	12.902387
13.204907	707.039092	12.907405
13.702367	701.390583	12.912423
13.399918	706.183364	12.917440
13.840841	702.650390	12.922458
13.351440	708.493359	12.927475
13.344465	699.276626	12.932493
13.412838	706.954679	12.937511
13.363346	703.165530	12.942528
13.508928	706.106276	12.947546
13.071712	711.008771	12.952563
13.254772	699.575659	12.957581
13.395368	699.229631	12.962599
13.214824	700.124110	12.967616
13.364288	698.459370	12.972634
13.301933	702.996265	12.977651
13.516959	697.978741	12.982669
13.598720	705.781341	12.987687
13.166509	699.591538	12.992704
13.469422	691.833248	12.997722
13.159753	701.188761	13.002739
13.319525	703.356731	13.007757
13.427172	706.377770	13.012775
13.336106	702.439609	13.017792
13.824552	710.129990	13.022810
13.791330	724.417007	13.027827
13.801661	717.358689	13.032845
13.443315	705.121575	13.037863
13.569382	721.686407	13.042880
13.702428	714.285742	13.047898
13.909355	726.960648	13.052915
13.706691	716.087035	13.057933
13.809398	711.285732	13.062951
13.491445	700.666640	13.067968
14.130607	711.188589	13.072986
13.754928	711.500062	13.078003
13.848110	694.983318	13.083021
13.830283	695.830776	13.088039
13.505419	693.449743	13.093056
14.002573	704.528241	13.098074
13.818149	703.009727	13.103091
13.958173	697.471977	13.108109
13.667673	698.508671	13.113127
13.368644	699.395212	13.118144
14.067265	709.433326	13.123162
13.990867	730.784564	13.128179
13.964870	716.586612	13.133197
14.018574	716.517162	13.138215
13.495537	724.535264	13.143232
14.105265	723.212394	13.148250
13.951695	731.386238	13.153267
13.858527	715.326684	13.158285
14.061759	716.380044	13.163303
13.620029	723.337894	13.168320
13.911026	720.560802	13.173338
13.945579	728.460989	13.178355
13.958909	728.975749	13.183373
14.087106	721.906179	13.188391
13.832805	721.349965	13.193408
13.964803	714.261267	13.198426
13.896479	722.421778	13.203443
13.828754	712.454510	13.208461
13.913221	729.231739	13.213479
13.583840	733.057391	13.218496
14.128614	739.588133	13.223514
13.742815	755.551578	13.228531
14.219441	755.642005	13.233549
14.304152	752.916388	13.238567
14.021537	759.225107	13.243584
14.271149	753.464084	13.248602
14.261229	761.463773	13.253619
14.309030	757.263640	13.258637
14.616493	761.109823	13.263655
14.344468	759.982559	13.268672
14.619202	751.554140	13.273690
14.520800	760.643222	13.278707
14.308721	754.468125	13.283725
14.665440	753.838685	13.288743
14.548592	752.928232	13.293760
14.511269	732.932468	13.298778
14.226449	730.145610	13.303795
14.493468	719.694193	13.308813
14.238517	719.164463	13.313831
14.275676	736.828617	13.318848
14.489937	740.942969	13.323866
14.213537	756.648551	13.328883
14.407723	739.202094	13.333901
14.746427	749.604540	13.338919
14.488678	758.415692	13.343936
14.670642	756.299132	13.348954
14.659347	745.016667	13.353971
14.769751	741.948627	13.358989
14.603928	738.712166	13.364007
14.812493	742.210175	13.369024
14.523033	724.768233	13.374042
14.179380	725.023619	13.379059
14.357418	745.437129	13.384077
14.953179	734.986775	13.389095
14.815920	751.292504	13.394112
14.859975	745.114760	13.399130
14.940181	746.664845	13.404147
14.173905	742.795173	13.409165
14.941350	734.340293	13.414183
14.547424	749.221281	13.419200
15.093942	743.229220	13.424218
14.985894	753.539904	13.429235
14.738503	740.597419	13.434253
15.100269	724.030660	13.439271
14.482467	724.157829	13.444288
14.851494	722.737815	13.449306
14.916373	735.072884	13.454323
14.859470	744.105482	13.459341
14.878976	742.596893	13.464359
14.584194	744.698412	13.469376
15.163296	745.141142	13.474394
15.178840	743.259215	13.479411
14.642443	737.075626	13.484429
14.873956	737.372379	13.489447
14.685761	747.625469	13.494464
15.074773	742.073244	13.499482
15.116943	751.188254	13.504499
15.528397	756.596656	13.509517
15.042322	735.391015	13.514535
14.695127	724.430311	13.519552
14.829438	718.302196	13.524570
14.736771	740.385626	13.529587
14.675931	746.772965	13.534605
15.180683	739.649302	13.539623
15.110202	745.975643	13.544640
15.007587	743.589689	13.549658
15.026677	746.219517	13.554675
14.827761	744.016823	13.559693
15.148578	751.864503	13.564711
14.693632	750.780914	13.569728
14.801234	750.999371	13.574746
14.931575	748.335880	13.579763
15.208608	775.968064	13.584781
15.289981	777.343952	13.589799
15.261021	781.985177	13.594816
15.507217	770.240394	13.599834
15.678984	774.009056	13.604851
15.242311	772.660642	13.609869
15.339531	762.780196	13.614887
15.192009	764.978587	13.619904
15.532916	768.855847	13.624922
16.042515	763.958807	13.629939
15.619968	752.046047	13.634957
15.386317	754.319719	13.639975
15.197644	743.291810	13.644992
15.066677	748.468390	13.650010
15.490034	748.277497	13.655027
15.260592	758.841738	13.660045
15.542074	762.194220	13.665063
15.405441	769.259830	13.670080
15.532409	778.402544	13.675098
15.722591	772.446642	13.680115
15.694698	764.947412	13.685133
15.458073	750.042222	13.690151
15.572420	762.683277	13.695168
15.609973	759.023000	13.700186
15.760485	767.253592	13.705203
15.350616	756.542207	13.710221
15.650297	756.237942	13.715239
15.553390	771.032763	13.720256
15.741178	770.297445	13.725274
15.977829	766.320355	13.730291
15.519953	776.687407	13.735309
15.618955	775.587676	13.740327
15.663980	774.638608	13.745344
15.540097	764.615649	13.750362
15.876257	777.600675	13.755379
15.611628	773.235748	13.760397
16.022205	769.772348	13.765415
15.830616	777.511198	13.770432
15.572005	764.028061	13.775450
15.792040	763.223233	13.780467
15.749003	776.438361	13.785485
15.833698	775.013852	13.790503
15.949896	768.269065	13.795520
15.813355	773.280444	13.800538
15.874272	771.848456	13.805555
15.995547	773.674404	13.810573
15.961365	775.066671	13.815591
15.999098	774.004643	13.820608
16.092382	772.959400	13.825626
16.333074	772.744819	13.830643
15.910980	768.437856	13.835661
16.051005	765.770395	13.840679
15.834693	777.804441	13.845696
15.562724	774.676488	13.850714
15.789566	770.254983	13.855731
15.614231	771.224190	13.860749
15.744638	772.606918	13.865767
15.982267	791.702819	13.870784
16.162032	798.021207	13.875802
16.086672	794.520555	13.880819
15.912643	801.482928	13.885837
16.221861	788.004560	13.890855
16.116196	794.065894	13.895872
16.124044	805.120768	13.900890
16.033051	804.257997	13.905907
16.024097	811.113123	13.910925
16.280551	804.237622	13.915943
16.035975	812.220290	13.920960
16.036166	804.899058	13.925978
15.981647	802.346478	13.930995
16.403454	809.610960	13.936013
16.250645	810.251259	13.941031
16.393959	815.358430	13.946048
16.757750	819.962978	13.951066
16.632435	805.412905	13.956083
16.609138	796.371248	13.961101
16.395145	802.978055	13.966119
16.592081	796.355312	13.971136
16.435827	798.707507	13.976154
16.678062	799.664262	13.981171
16.229696	806.780720	13.986189
16.746943	791.891597	13.991207
16.334415	794.453934	13.996224
16.289751	799.290274	14.001242
16.615499	806.049428	14.006259
16.858280	816.703616	14.011277
16.839764	808.389863	14.016295
16.930913	801.014597	14.021312
16.481676	798.924994	14.026330
16.885570	789.644109	14.031347
16.554123	793.722072	14.036365
16.419085	796.454198	14.041383
16.728098	795.406695	14.046400
16.881531	795.385687	14.051418
16.580301	784.291352	14.056435
16.578632	794.458472	14.061453
16.743121	815.952607	14.066471
16.864209	817.106580	14.071488
16.827778	825.413037	14.076506
17.168440	820.739219	14.081523
16.673174	806.755496	14.086541
16.657876	805.364470	14.091559
17.024244	812.125561	14.096576
16.948306	815.875410	14.101594
17.010580	816.535210	14.106611
17.138145	829.878819	14.111629
17.033766	815.176459	14.116647
16.956838	801.613602	14.121664
16.446722	801.519800	14.126682
16.985064	805.054157	14.131699
17.112632	827.323279	14.136717
17.065219	824.207343	14.141735
16.630001	820.010012	14.146752
16.805875	826.804622	14.151770
17.060416	817.727576	14.156787
16.867164	825.752143	14.161805
16.963069	821.374351	14.166823
16.951127	825.103763	14.171840
16.720502	825.340041	14.176858
17.148035	815.957987	14.181875
17.050564	819.171667	14.186893
17.104913	817.487232	14.191911
17.177036	817.891871	14.196928
17.055773	832.917545	14.201946
17.613463	845.406914	14.206963
17.425034	841.340358	14.211981
17.327301	816.248842	14.216999
17.578493	821.813325	14.222016
17.275566	824.131940	14.227034
17.389081	816.032922	14.232051
17.254142	819.571292	14.237069
17.151297	807.328401	14.242087
17.478591	818.763437	14.247104
17.312103	819.081215	14.252122
17.611245	814.177672	14.257139
17.639639	824.396130	14.262157
17.440539	812.261295	14.267175
17.823761	820.593926	14.272192
17.382851	812.581203	14.277210
17.469397	813.455083	14.282227
17.598141	810.343443	14.287245
17.354102	804.435021	14.292263
17.670014	818.447790	14.297280
17.385050	822.885761	14.302298
17.626961	825.292103	14.307315
17.828411	832.561195	14.312333
17.898505	828.068784	14.317351
17.944208	819.075921	14.322368
17.940130	821.732826	14.327386
17.833386	806.148235	14.332403
17.577505	806.701276	14.337421
17.528308	804.374968	14.342439
17.731463	809.379320	14.347456
17.603600	809.211988	14.352474
17.338870	814.563093	14.357491
17.395421	828.039319	14.362509
17.729459	829.575333	14.367527
17.773236	831.154291	14.372544
17.373898	843.385221	14.377562
17.851248	834.101989	14.382579
17.646568	836.162617	14.387597
17.877711	845.636923	14.392615
18.122711	835.710308	14.397632
17.899378	835.419027	14.402650
17.944637	835.390342	14.407667
17.865291	831.230927	14.412685
17.960084	841.294314	14.417703
18.016241	831.131662	14.422720
17.692418	838.960939	14.427738
17.968987	843.704733	14.432755
18.407672	859.206189	14.437773
18.618174	849.571484	14.442791
18.655512	836.353043	14.447808
18.549196	836.701407	14.452826
18.270508	821.424392	14.457843
18.113795	834.675321	14.462861
17.814396	829.414212	14.467879
18.248052	823.196727	14.472896
17.970369	837.967612	14.477914
18.105221	831.342931	14.482931
18.393262	825.401905	14.487949
18.378972	833.326374	14.492967
18.260753	823.328815	14.497984
18.533077	837.058282	14.503002
18.625062	818.531471	14.508019
18.384014	817.334903	14.513037
18.475239	829.617262	14.518055
18.545665	828.447854	14.523072
18.446520	830.049691	14.528090
18.513370	820.907270	14.533107
18.397784	820.313517	14.538125
18.395593	824.574751	14.543143
18.655568	825.125836	14.548160
18.564737	830.074155	14.553178
18.348805	833.555865	14.558195
18.813233	823.448443	14.563213
18.355850	826.360321	14.568231
18.498417	825.584852	14.573248
18.627799	829.160556	14.578266
18.489900	823.471941	14.583283
18.233005	825.558930	14.588301
18.227339	826.156756	14.593319
18.526238	832.784941	14.598336
18.695629	830.271261	14.603354
18.494454	843.920485	14.608371
18.788596	851.059283	14.613389
18.523364	845.370091	14.618407
19.075094	858.286421	14.623424
18.804435	859.862333	14.628442
18.936629	860.134986	14.633459
18.635931	863.855924	14.638477
18.759067	852.660564	14.643495
18.788390	847.439502	14.648512
18.901953	860.953558	14.653530
18.919289	860.503140	14.658547
19.417078	852.467632	14.663565
18.869211	863.003571	14.668583
19.299690	848.848805	14.673600
18.993005	849.520884	14.678618
18.945675	848.829218	14.683635
18.897839	838.063340	14.688653
19.204408	853.798860	14.693671
19.419920	853.476249	14.698688
19.026184	844.457716	14.703706
18.830641	827.568976	14.708723
19.127603	835.539147	14.713741
18.622614	842.336666	14.718759
19.243693	842.658281	14.723776
19.275804	851.071114	14.728794
18.930928	856.355194	14.733811
19.195014	850.996050	14.738829
18.980919	859.985062	14.743847
19.341549	855.674838	14.748864
19.363593	850.323096	14.753882
19.456816	845.227274	14.758899
19.451518	848.775286	14.763917
18.970787	853.256704	14.768935
18.940341	849.944656	14.773952
19.061868	857.131723	14.778970
19.039547	855.858779	14.783987
19.399901	850.054582	14.789005
19.377844	852.845171	14.794023
19.564254	843.043602	14.799040
19.309498	846.670713	14.804058
19.687222	856.643956	14.809075
19.548050	848.735180	14.814093
19.349999	858.606530	14.819111
19.438733	850.745444	14.824128
19.474294	861.904031	14.829146
19.597333	879.876159	14.834163
19.807084	875.208254	14.839181
19.533189	867.653257	14.844199
19.925698	865.429775	14.849216
19.613689	848.975631	14.854234
19.602544	852.772631	14.859251
19.985115	843.920420	14.864269
19.598962	858.806919	14.869287
19.744552	849.307366	14.874304
19.557457	847.998717	14.879322
19.434986	866.765382	14.884339
19.979686	879.815171	14.889357
19.890601	877.016346	14.894375
19.923322	888.969479	14.899392
20.152159	888.230114	14.904410
19.699907	874.433685	14.909427
19.963140	864.948499	14.914445
19.944650	876.685311	14.919463
20.040067	874.005535	14.924480
20.217499	875.257264	14.929498
20.135715	863.308858	14.934515
20.160035	850.679932	14.939533
19.665672	858.275266	14.944551
19.708943	849.780008	14.949568
20.157937	865.612817	14.954586
20.041408	885.262336	14.959603
20.277282	876.093076	14.964621
20.057079	878.708222	14.969639
20.196316	879.791480	14.974656
20.153894	875.490513	14.979674
20.129105	880.188160	14.984691
20.365423	878.320052	14.989709
20.241103	884.580564	14.994727
20.203120	874.828335	14.999744
20.357286	874.020236	15.004762
20.222700	877.977833	15.009779
20.407791	865.711232	15.014797
20.606207	875.349235	15.019815
20.494536	874.881204	15.024832
20.403946	852.358794	15.029850
20.128887	872.715222	15.034867
20.472093	871.211680	15.039885
20.181206	875.051069	15.044903
20.220284	875.141119	15.049920
20.578312	873.501664	15.054938
20.309388	876.909092	15.059955
20.406279	878.056052	15.064973
20.243123	875.873400	15.069991
20.539326	877.342459	15.075008
20.714366	876.478150	15.080026
20.375208	873.094386	15.085043
20.284841	874.787683	15.090061
20.515792	878.180840	15.095079
20.093593	873.696706	15.100096
20.613533	878.344311	15.105114
20.357221	893.255797	15.110131
20.458897	894.168513	15.115149
20.416350	898.028988	15.120167
20.656329	901.775363	15.125184
20.981354	892.422442	15.130202
20.786620	896.947064	15.135219
21.128682	893.032405	15.140237
20.932439	894.740086	15.145255
20.961586	894.251492	15.150272
21.084015	893.696274	15.155290
20.910452	897.394594	15.160307
21.412450	900.210616	15.165325
20.962265	898.264456	15.170343
20.873615	905.009598	15.175360
21.163300	902.007505	15.180378
21.100152	902.321953	15.185395
20.792447	886.357977	15.190413
20.336738	886.724828	15.195431
20.674775	888.270815	15.200448
21.026183	892.837280	15.205466
20.892683	894.509770	15.210483
21.042601	906.197459	15.215501
21.039658	900.756929	15.220519
20.958511	890.713032	15.225536
21.300070	890.112474	15.230554
20.836303	896.308338	15.235571
21.036987	896.452727	15.240589
21.249181	917.104497	15.245607
21.134790	918.524624	15.250624
21.244661	912.124901	15.255642
21.386404	928.227538	15.260659
21.189153	921.894019	15.265677
21.463750	922.619844	15.270695
21.170148	922.277994	15.275712
21.529528	916.680617	15.280730
21.078807	923.518396	15.285747
21.710481	921.194678	15.290765
21.656251	926.491676	15.295783
21.866610	917.399842	15.300800
21.777300	916.852913	15.305818
21.748304	924.098792	15.310835
22.155146	918.660871	15.315853
21.814177	893.461480	15.320871
21.669894	889.786401	15.325888
21.736147	883.461232	15.330906
21.425462	879.346015	15.335923
21.591448	879.445758	15.340941
21.846578	884.155322	15.345959
21.646143	889.661547	15.350976
21.680168	887.522617	15.355994
21.501244	893.602026	15.361011
21.518189	917.023794	15.366029
21.877159	914.279899	15.371047
21.571061	921.071683	15.376064
22.013340	904.993345	15.381082
21.850968	914.694264	15.386099
21.674364	910.243071	15.391117
22.010714	918.494546	15.396135
21.992695	913.891115	15.401152
22.095993	912.347376	15.406170
22.090887	915.284770	15.411187
21.986242	915.650181	15.416205
22.228521	920.059929	15.421223
22.147034	922.011197	15.426240
22.714362	912.587829	15.431258
22.426678	922.411072	15.436275
22.465220	900.671898	15.441293
22.209481	880.270397	15.446311
21.874133	877.167484	15.451328
22.141904	880.264401	15.456346
21.757537	889.885532	15.461363
22.236625	900.630566	15.466381
22.180178	912.475654	15.471399
22.209446	916.906106	15.476416
22.648461	912.472262	15.481434
22.383928	914.962871	15.486451
22.318042	914.640793	15.491469
22.561787	911.728585	15.496487
22.421474	923.084048	15.501504
22.272571	905.361946	15.506522
22.436076	918.788653	15.511539
22.380941	909.512055	15.516557
22.864333	912.461864	15.521575
22.601931	916.824869	15.526592
22.464361	901.064192	15.531610
22.411795	904.478711	15.536627
22.402834	905.923109	15.541645
22.454518	912.425343	15.546663
22.272884	914.319181	15.551680
22.426649	906.148100	15.556698
22.395250	915.121065	15.561715
22.204824	914.709771	15.566733
22.407547	910.809520	15.571751
22.223341	917.556317	15.576768
22.665829	919.340513	15.581786
22.504781	936.282236	15.586803
22.632190	935.519114	15.591821
22.991410	935.589617	15.596839
22.814472	940.891191	15.601856
23.143630	931.979668	15.606874
22.957555	929.120125	15.611891
23.050243	926.112854	15.616909
23.377633	930.723857	15.621927
22.966937	938.777008	15.626944
23.220835	917.611179	15.631962
23.018393	909.574271	15.636979
22.654779	914.536291	15.641997
23.154608	919.689184	15.647015
22.901041	926.292360	15.652032
23.308347	919.837084	15.657050
23.242739	929.617654	15.662067
23.094961	926.133688	15.667085
23.398201	926.515808	15.672103
23.144444	925.751631	15.677120
23.265950	920.220412	15.682138
23.322527	927.281265	15.687155
23.142045	926.152609	15.692173
23.369096	924.617904	15.697191
23.447172	927.806081	15.702208
23.475512	928.221910	15.707226
23.209783	925.825537	15.712243
23.106916	931.787254	15.717261
23.290573	929.351113	15.722279
23.033857	938.491316	15.727296
23.357326	924.487658	15.732314
23.465475	924.843424	15.737331
23.315771	928.742122	15.742349
23.610921	925.756048	15.747367
23.692743	933.155228	15.752384
23.477295	922.500112	15.757402
23.454644	928.741052	15.762419
23.505669	928.907860	15.767437
23.796215	920.143676	15.772455
23.396726	927.478856	15.777472
23.445852	919.680197	15.782490
23.381881	928.893198	15.787507
23.445051	939.040228	15.792525
23.783366	950.696756	15.797543
23.665290	961.843849	15.802560
23.602257	955.923113	15.807578
23.926853	964.769053	15.812595
23.869092	957.877011	15.817613
24.035839	954.594097	15.822631
24.177401	956.304902	15.827648
24.231098	946.046130	15.832666
24.359264	954.660427	15.837683
23.902922	943.854248	15.842701
24.416155	925.516207	15.847719
23.925127	928.357693	15.852736
23.868714	914.957867	15.857754
23.917812	918.363429	15.862771
24.142805	930.472151	15.867789
24.306214	930.654601	15.872807
23.976389	933.208777	15.877824
24.358910	941.349080	15.882842
24.217872	936.900258	15.887859
24.203689	929.354979	15.892877
24.148827	922.853007	15.897895
23.966411	933.262736	15.902912
24.475413	941.744678	15.907930
24.544274	949.647565	15.912947
24.183056	950.017274	15.917965
24.406874	936.481267	15.922983
24.094555	945.677923	15.928000
24.243901	943.249037	15.933018
24.149832	949.591964	15.938035
24.182740	948.189006	15.943053
24.031238	942.373471	15.948071
23.929121	948.155943	15.953088
24.207391	948.104817	15.958106
24.529487	954.361907	15.963123
24.531349	966.513903	15.968141
24.652739	973.277837	15.973159
24.748194	971.183447	15.978176
24.606781	965.068607	15.983194
24.795120	960.324698	15.988211
24.598340	958.375938	15.993229
24.768661	952.868119	15.998247
24.991723	958.655804	16.003264
24.789240	960.244451	16.008282
25.020407	963.638773	16.013299
24.802897	959.932103	16.018317
24.871462	952.019977	16.023335
24.919358	964.900932	16.028352
24.939271	964.054038	16.033370
25.057959	959.603933	16.038387
24.685187	960.895595	16.043405
25.219619	958.594666	16.048423
24.910473	957.878240	16.053440
24.621794	951.026012	16.058458
24.988495	961.452705	16.063475
24.949298	966.933046	16.068493
25.087960	966.660952	16.073511
24.939605	959.904378	16.078528
25.091359	964.671240	16.083546
24.925361	960.408820	16.088563
24.766495	964.155113	16.093581
25.504788	967.412711	16.098599
25.301952	969.534466	16.103616
25.417636	966.767857	16.108634
25.262961	957.147097	16.113651
25.112450	956.846117	16.118669
25.330997	974.578142	16.123687
25.389633	980.434792	16.128704
25.637087	988.172305	16.133722
25.488341	982.007494	16.138739
25.392364	984.861920	16.143757
25.789978	981.939575	16.148775
25.607982	977.040061	16.153792
25.110418	972.878601	16.158810
25.599956	978.329268	16.163827
25.529959	987.741719	16.168845
25.810794	985.085551	16.173863
25.816061	992.715930	16.178880
25.880338	986.837485	16.183898
26.224340	975.214929	16.188915
25.799938	975.004181	16.193933
25.864316	957.810852	16.198951
25.636779	953.986952	16.203968
25.489919	951.341768	16.208986
25.840597	945.868257	16.214003
25.542431	960.721387	16.219021
25.952908	965.416277	16.224039
26.030639	989.540264	16.229056
25.971429	982.609476	16.234074
25.680350	984.493493	16.239091
25.961194	991.390081	16.244109
26.014249	976.681970	16.249127
26.126065	979.137830	16.254144
25.798453	978.652403	16.259162
26.118097	983.845783	16.264179
26.063839	984.719760	16.269197
26.218151	981.147967	16.274215
26.209738	987.820019	16.279232
25.903870	984.684250	16.284250
26.105763	983.324565	16.289267
25.880489	981.492721	16.294285
26.099238	980.105443	16.299303
26.137103	981.398400	16.304320
25.901159	987.122341	16.309338
26.199391	991.591740	16.314355
26.214157	1010.343728	16.319373
26.669088	1011.149141	16.324391
26.654889	1006.178136	16.329408
26.416364	1008.797124	16.334426
26.587515	1010.006993	16.339443
26.651920	1014.139540	16.344461
26.648338	1003.287088	16.349479
26.717055	994.189924	16.354496
26.621168	983.832671	16.359514
26.739210	980.363336	16.364531
26.493849	976.117596	16.369549
26.384844	982.129165	16.374567
26.432586	1002.577976	16.379584
26.220031	999.972007	16.384602
26.424599	1006.996581	16.389619
26.723638	1012.157557	16.394637
26.753548	1008.920517	16.399655
26.715969	1008.440212	16.404672
26.359544	999.309508	16.409690
27.045029	1007.327242	16.414707
26.834844	1006.868038	16.419725
26.908932	1009.404557	16.424743
27.009042	1019.074676	16.429760
27.123264	1029.366456	16.434778
27.245490	1024.342147	16.439795
26.872398	1016.225964	16.444813
27.192591	1021.546033	16.449831
27.594432	1024.025921	16.454848
27.174406	1014.946288	16.459866
26.905091	1003.304405	16.464883
27.142111	1008.040233	16.469901
27.048648	1013.462257	16.474919
27.400043	1029.231084	16.479936
27.389380	1029.426611	16.484954
27.706410	1016.260519	16.489971
27.394303	1012.370296	16.494989
27.231733	996.532168	16.500007
27.095848	995.432734	16.505024
27.221299	1013.586895	16.510042
27.397743	1015.069892	16.515059
27.505226	1020.585018	16.520077
27.611781	1015.067657	16.525095
27.434487	1027.598565	16.530112
27.239516	1023.221244	16.535130
27.802754	1021.934395	16.540147
27.658709	1030.328859	16.545165
27.598607	1021.878181	16.550183
27.470507	1019.188542	16.555200
27.515001	1025.425095	16.560218
27.726495	1015.580682	16.565235
27.801648	1016.822194	16.570253
27.509663	1023.264062	16.575271
27.800414	1019.299997	16.580288
27.716034	1027.224754	16.585306
27.721088	1016.682268	16.590323
27.619635	1018.582920	16.595341
27.831460	1018.760503	16.600359
27.908711	1009.808367	16.605376
27.553628	1028.298009	16.610394
28.291835	1025.644050	16.615411
27.968946	1031.709557	16.620429
27.880049	1033.403809	16.625447
28.078651	1031.291543	16.630464
28.058627	1048.541916	16.635482
28.282911	1045.149853	16.640499
28.377752	1043.350032	16.645517
28.258742	1050.167191	16.650535
28.404247	1051.331705	16.655552
27.872221	1034.953554	16.660570
28.203392	1039.269880	16.665587
28.040326	1043.955830	16.670605
28.285389	1042.246485	16.675623
28.285673	1042.120526	16.680640
28.035635	1044.320970	16.685658
28.046320	1038.001396	16.690675
28.229513	1042.655206	16.695693
28.030487	1041.870544	16.700711
28.443800	1045.785097	16.705728
28.488855	1054.680525	16.710746
28.952216	1063.132298	16.715763
29.218825	1045.364855	16.720781
28.450037	1042.334071	16.725799
28.679751	1035.181017	16.730816
28.800785	1026.862148	16.735834
28.639785	1021.719390	16.740851
28.912040	1025.690757	16.745869
28.470969	1029.040504	16.750887
28.773077	1027.325258	16.755904
28.437862	1039.627610	16.760922
28.785737	1050.847609	16.765939
28.890452	1056.092349	16.770957
29.154258	1061.706010	16.775975
29.131499	1056.948603	16.780992
28.948584	1059.815075	16.786010
29.067336	1050.808408	16.791027
29.487223	1052.419597	16.796045
29.097805	1047.983524	16.801063
29.109958	1034.339179	16.806080
29.040299	1035.583805	16.811098
28.758339	1046.923444	16.816115
29.370207	1056.791909	16.821133
29.103540	1059.629338	16.826151
29.328952	1055.169015	16.831168
29.320271	1057.463743	16.836186
29.265402	1057.666590	16.841203
29.360050	1058.711578	16.846221
29.229358	1055.163731	16.851239
29.397723	1055.496931	16.856256
29.324094	1064.990343	16.861274
29.245881	1067.396583	16.866291
29.438500	1068.932417	16.871309
29.157047	1064.194221	16.876327
29.788498	1055.237298	16.881344
29.358007	1061.367876	16.886362
29.727391	1047.336033	16.891379
29.624940	1046.921191	16.896397
29.421484	1051.889805	16.901415
29.459647	1056.877465	16.906432
29.168989	1055.880817	16.911450
29.436304	1057.135001	16.916467
29.927278	1069.356871	16.921485
29.644957	1079.647025	16.926503
29.844558	1080.489602	16.931520
29.987820	1081.227339	16.936538
30.223004	1077.588592	16.941555
30.320511	1061.865988	16.946573
29.817329	1055.033091	16.951591
29.877570	1047.617158	16.956608
30.131879	1061.244301	16.961626
29.855572	1068.798905	16.966643
30.358498	1069.292842	16.971661
30.060900	1065.415162	16.976679
30.119377	1049.828951	16.981696
30.229379	1055.357451	16.986714
30.313356	1064.279509	16.991731
30.450460	1067.970128	16.996749
29.995374	1065.120852	17.001767
30.313709	1051.900185	17.006784
30.367162	1070.395850	17.011802
30.316230	1070.053970	17.016819
30.413966	1067.060008	17.021837
30.584257	1074.044622	17.026855
30.547071	1066.270022	17.031872
30.331165	1073.515819	17.036890
30.375338	1077.689921	17.041907
30.567321	1060.098986	17.046925
30.279643	1073.082444	17.051943
30.601075	1078.768457	17.056960
30.663761	1072.750483	17.061978
30.225066	1078.552516	17.066995
30.747818	1060.170616	17.072013
30.566198	1070.002767	17.077031
30.483362	1071.120449	17.082048
30.412796	1068.316947	17.087066
30.653858	1068.531028	17.092083
30.843759	1063.981704	17.097101
30.734335	1081.465019	17.102119
30.814811	1092.822234	17.107136
31.115135	1095.411461	17.112154
30.999362	1099.553393	17.117171
31.537246	1093.646485	17.122189
31.050015	1084.964539	17.127207
30.845215	1069.962040	17.132224
30.823583	1070.193634	17.137242
30.935989	1092.169597	17.142259
31.362095	1091.382992	17.147277
31.014207	1098.960881	17.152295
31.570088	1091.936464	17.157312
31.490824	1091.150078	17.162330
31.363839	1082.302187	17.167347
31.644568	1079.820818	17.172365
31.139696	1073.947213	17.177383
31.143491	1077.431175	17.182400
31.432168	1086.186680	17.187418
31.241479	1089.986303	17.192435
31.527157	1085.426625	17.197453
31.480605	1092.162122	17.202471
31.430812	1085.629322	17.207488
31.554365	1084.658965	17.212506
31.614623	1087.104088	17.217523
31.944409	1084.283504	17.222541
31.438845	1090.300937	17.227559
31.571160	1090.086583	17.232576
31.552232	1090.048448	17.237594
31.338257	1081.610618	17.242611
31.837199	1083.362652	17.247629
31.969736	1093.656167	17.252647
31.732792	1084.300517	17.257664
31.760519	1084.052695	17.262682
31.375322	1089.158496	17.267699
31.635110	1079.816265	17.272717
31.688007	1090.226898	17.277735
31.981758	1105.647487	17.282752
32.058429	1107.462752	17.287770
32.094989	1120.300833	17.292787
32.227508	1112.442600	17.297805
31.985846	1114.062158	17.302823
32.408397	1107.821991	17.307840
32.312119	1113.359866	17.312858
32.393943	1114.384540	17.317875
32.012394	1113.642694	17.322893
31.970600	1107.428628	17.327911
32.492194	1118.873053	17.332928
32.314178	1111.759918	17.337946
32.359056	1116.141781	17.342963
32.495508	1114.124832	17.347981
32.658398	1123.715333	17.352999
32.505135	1116.410701	17.358016
32.467473	1108.720014	17.363034
32.266258	1114.432346	17.368051
32.852430	1109.676060	17.373069
32.475743	1113.684433	17.378087
32.453571	1106.442349	17.383104
32.410599	1102.331167	17.388122
32.397020	1107.901407	17.393139
32.496571	1102.796579	17.398157
32.652282	1125.814990	17.403175
32.913381	1134.901456	17.408192
33.173743	1131.071525	17.413210
32.775267	1136.519293	17.418227
33.046419	1123.676445	17.423245
33.230508	1131.445389	17.428263
33.036312	1118.230793	17.433280
32.982654	1111.813579	17.438298
32.962786	1129.143934	17.443315
33.452700	1129.912855	17.448333
33.203463	1115.898739	17.453351
32.915254	1114.372171	17.458368
33.318151	1112.400866	17.463386
33.203488	1131.124040	17.468403
33.618542	1131.143569	17.473421
33.406044	1121.739754	17.478439
33.144085	1111.056777	17.483456
33.246918	1111.183907	17.488474
33.159747	1127.160095	17.493491
33.193123	1134.299686	17.498509
33.514458	1136.951580	17.503527
33.222386	1134.261513	17.508544
33.377271	1130.786831	17.513562
33.238816	1129.428373	17.518579
33.556443	1134.191050	17.523597
33.482771	1129.714876	17.528615
33.441286	1127.496687	17.533632
33.726622	1138.768443	17.538650
33.341244	1132.024269	17.543667
33.637195	1133.909917	17.548685
33.615378	1147.496640	17.553703
33.755725	1161.586035	17.558720
34.024601	1155.063430	17.563738
34.038279	1155.054541	17.568755
34.480297	1146.115941	17.573773
33.970865	1134.062944	17.578791
33.733458	1125.404567	17.583808
33.947954	1127.606842	17.588826
33.745356	1142.747855	17.593843
33.868157	1148.658510	17.598861
34.009400	1144.807356	17.603879
34.421232	1147.480093	17.608896
34.315761	1143.982378	17.613914
34.061688	1151.645149	17.618931
34.323074	1142.440407	17.623949
34.718405	1144.284012	17.628967
34.662118	1139.297098	17.633984
34.777151	1141.672139	17.639002
34.716900	1138.225992	17.644019
34.406315	1122.760263	17.649037
34.301249	1124.709949	17.654055
34.484111	1140.398533	17.659072
34.334820	1133.770379	17.664090
34.215493	1146.165411	17.669107
34.787180	1134.980612	17.674125
34.658770	1142.001330	17.679143
34.298918	1138.674868	17.684160
34.807524	1139.512345	17.689178
34.446519	1144.309837	17.694195
34.690404	1140.892856	17.699213
34.896837	1140.641426	17.704231
34.760263	1136.112282	17.709248
34.899532	1133.019701	17.714266
34.717749	1135.438377	17.719283
34.797268	1136.766574	17.724301
34.827871	1140.774048	17.729319
34.903748	1153.999729	17.734336
34.910735	1165.721519	17.739354
35.175637	1166.819029	17.744371
35.370236	1163.449966	17.749389
35.581173	1157.014904	17.754407
35.638580	1161.869101	17.759424
35.552886	1130.637862	17.764442
35.165052	1131.752901	17.769459
35.072245	1123.100503	17.774477
35.080252	1130.407279	17.779495
35.174508	1148.634873	17.784512
35.582115	1155.481412	17.789530
35.492353	1164.219705	17.794547
35.847340	1151.291695	17.799565
35.865242	1154.767827	17.804583
35.571132	1154.521328	17.809600
35.706538	1159.515360	17.814618
35.467175	1157.005532	17.819635
35.716669	1153.064406	17.824653
35.765737	1154.607877	17.829671
35.579927	1154.196206	17.834688
35.760529	1150.030668	17.839706
35.581369	1151.661534	17.844723
35.911818	1162.518370	17.849741
35.822032	1157.578728	17.854759
35.618612	1150.043416	17.859776
36.110053	1153.930494	17.864794
35.888007	1157.393604	17.869811
35.971216	1160.468384	17.874829
36.107041	1157.173226	17.879847
35.572606	1164.818254	17.884864
36.053560	1154.298446	17.889882
35.794499	1161.860475	17.894899
36.235543	1180.874755	17.899917
36.560432	1176.237301	17.904935
36.382449	1176.403449	17.909952
36.484770	1176.990495	17.914970
36.279476	1162.726548	17.919987
36.368429	1173.043474	17.925005
36.439719	1173.766362	17.930023
36.399510	1180.456754	17.935040
36.467782	1179.374288	17.940058
36.671630	1181.129528	17.945075
36.477333	1184.964416	17.950093
36.646816	1176.279975	17.955111
36.399234	1179.204420	17.960128
36.624575	1174.547624	17.965146
36.873557	1176.806005	17.970163
36.561670	1173.512143	17.975181
36.519688	1171.727088	17.980199
36.341553	1181.372517	17.985216
36.822192	1170.056711	17.990234
37.000004	1181.282918	17.995251
36.820115	1180.826959	18.000269
37.003365	1179.029805	18.005287
36.925004	1183.887986	18.010304
37.007186	1188.519985	18.015322
37.584316	1197.167557	18.020339
37.196003	1187.521561	18.025357
37.363776	1180.789708	18.030375
37.040266	1169.273598	18.035392
37.296985	1174.481006	18.040410
37.346507	1172.466633	18.045427
37.230158	1180.664865	18.050445
37.370212	1174.152953	18.055463
37.023840	1206.204363	18.060480
37.759403	1203.791753	18.065498
37.386079	1205.240607	18.070515
37.383308	1202.406958	18.075533
37.800668	1198.630934	18.080551
37.344956	1200.528850	18.085568
37.484330	1195.684713	18.090586
37.353560	1200.219302	18.095603
37.466287	1195.246116	18.100621
37.908935	1195.890981	18.105639
37.847677	1195.245305	18.110656
37.731286	1204.464394	18.115674
38.137158	1200.872944	18.120691
37.662970	1203.972312	18.125709
37.665572	1197.782354	18.130727
37.526468	1198.040488	18.135744
37.979310	1213.538384	18.140762
38.300114	1221.791809	18.145779
38.653776	1216.621247	18.150797
38.544642	1197.938704	18.155815
38.369436	1194.850546	18.160832
38.453335	1181.892203	18.165850
38.458357	1188.938485	18.170867
38.048832	1191.335431	18.175885
38.535728	1180.433923	18.180903
38.129643	1181.445692	18.185920
38.419965	1178.797763	18.190938
38.596622	1174.553741	18.195955
38.278877	1186.190736	18.200973
38.559690	1183.599497	18.205991
38.327377	1185.391919	18.211008
38.614175	1182.660717	18.216026
38.562847	1174.943127	18.221043
38.550073	1198.109226	18.226061
38.892301	1201.652530	18.231079
39.080012	1214.148741	18.236096
38.792063	1204.557768	18.241114
38.637447	1181.116371	18.246131
38.615128	1195.144545	18.251149
38.818652	1200.264709	18.256167
38.674410	1205.435372	18.261184
38.744537	1210.473693	18.266202
38.830744	1216.980181	18.271219
38.775957	1217.055068	18.276237
38.903705	1215.476544	18.281255
38.699489	1220.622497	18.286272
38.708682	1214.652301	18.291290
39.074205	1222.128264	18.296307
39.255273	1244.689910	18.301325
39.283135	1244.558202	18.306343
39.071894	1252.373375	18.311360
39.189534	1245.061620	18.316378
39.428111	1232.156362	18.321395
39.420890	1235.107945	18.326413
39.681584	1235.255394	18.331431
39.751924	1236.463470	18.336448
39.941712	1237.202960	18.341466
39.891898	1236.758137	18.346483
39.620282	1239.733816	18.351501
39.893370	1232.583725	18.356519
39.934104	1228.577543	18.361536
39.730212	1235.782057	18.366554
39.724345	1228.390369	18.371571
39.665001	1237.601213	18.376589
39.717031	1224.132770	18.381607
39.734725	1230.477778	18.386624
39.641852	1232.127041	18.391642
40.016956	1233.060644	18.396659
39.924037	1239.244054	18.401677
40.002584	1230.249845	18.406695
40.019160	1230.314096	18.411712
39.716501	1237.587719	18.416730
40.209697	1240.748957	18.421747
39.763119	1255.905282	18.426765
40.491775	1251.219061	18.431783
40.593028	1259.169497	18.436800
40.464998	1254.764097	18.441818
40.238276	1244.891314	18.446835
40.248153	1255.426895	18.451853
40.169870	1240.071005	18.456871
40.587042	1243.606241	18.461888
40.222813	1247.529516	18.466906
40.753279	1238.554565	18.471923
40.182724	1256.255373	18.476941
40.611712	1258.471757	18.481959
40.464215	1277.183615	18.486976
40.438365	1279.657594	18.491994
41.078624	1274.958443	18.497011
40.943464	1273.382502	18.502029
40.940792	1274.545585	18.507047
41.171834	1276.408142	18.512064
41.194406	1278.391042	18.517082
41.517667	1274.959314	18.522099
41.120659	1273.529483	18.527117
41.539206	1274.506681	18.532135
41.233408	1263.568657	18.537152
41.454058	1254.387522	18.542170
41.416360	1246.588114	18.547187
41.136480	1237.203653	18.552205
41.228838	1232.798775	18.557223
41.260554	1241.498493	18.562240
41.112895	1259.178886	18.567258
41.598368	1263.522483	18.572275
41.146568	1272.075906	18.577293
41.436691	1267.663074	18.582311
41.385902	1275.392243	18.587328
41.163693	1271.757534	18.592346
41.580838	1264.970968	18.597363
41.368402	1265.823515	18.602381
41.667828	1263.901607	18.607399
41.594154	1256.710892	18.612416
41.676771	1270.732783	18.617434
41.649452	1269.692122	18.622451
41.836882	1293.781886	18.627469
41.951055	1283.113672	18.632487
42.124204	1289.134546	18.637504
41.782949	1299.386572	18.642522
42.018875	1295.925206	18.647539
41.884156	1301.332902	18.652557
41.879488	1287.341913	18.657575
41.962274	1283.565756	18.662592
41.943963	1289.608096	18.667610
41.947138	1276.648866	18.672627
41.939726	1297.113892	18.677645
42.128506	1310.546993	18.682663
42.400373	1304.615551	18.687680
42.186756	1319.853047	18.692698
42.549807	1308.441259	18.697715
42.224799	1315.921764	18.702733
42.461636	1315.385383	18.707751
42.779540	1315.608398	18.712768
42.669680	1318.434082	18.717786
42.982457	1312.393109	18.722803
42.984280	1316.314057	18.727821
42.623697	1310.558985	18.732839
42.759046	1311.182299	18.737856
42.928165	1311.192159	18.742874
43.186172	1311.272338	18.747891
43.206631	1310.556828	18.752909
43.066777	1307.160437	18.757927
43.120758	1303.335110	18.762944
43.026010	1307.185040	18.767962
43.219211	1308.021604	18.772979
42.976723	1309.751159	18.777997
43.264529	1308.216988	18.783015
43.241852	1303.969717	18.788032
43.379345	1317.132974	18.793050
43.375622	1305.058311	18.798067
43.547573	1305.879890	18.803085
43.142992	1308.900038	18.808103
43.717964	1307.455717	18.813120
43.591458	1338.850537	18.818138
44.040592	1320.124228	18.823155
43.622207	1319.340044	18.828173
43.792347	1310.946752	18.833191
44.023932	1296.682389	18.838208
43.614222	1302.210419	18.843226
44.011238	1301.374293	18.848243
44.068412	1301.164505	18.853261
43.903583	1306.264202	18.858279
43.810659	1295.868061	18.863296
43.722138	1302.878309	18.868314
44.120601	1315.797572	18.873331
44.266615	1318.442702	18.878349
43.805421	1329.417349	18.883367
44.063819	1326.037294	18.888384
44.084379	1332.505883	18.893402
44.120608	1322.089520	18.898419
43.718575	1324.117929	18.903437
43.771089	1333.679594	18.908455
43.987851	1324.811260	18.913472
44.116437	1331.698174	18.918490
44.572125	1342.113542	18.923507
44.681209	1355.743732	18.928525
44.152948	1356.226144	18.933543
44.607669	1356.784768	18.938560
44.605561	1357.731625	18.943578
44.543405	1356.688066	18.948595
44.766996	1360.280578	18.953613
44.657747	1365.686047	18.958631
44.783647	1348.736031	18.963648
44.549491	1341.028552	18.968666
45.071563	1356.273008	18.973683
44.891020	1345.153559	18.978701
45.028098	1351.771757	18.983719
45.033166	1350.776122	18.988736
44.991833	1349.440144	18.993754
45.248284	1340.560112	18.998771
45.183894	1339.871248	19.003789
45.142500	1339.265976	19.008807
45.487897	1340.896225	19.013824
45.449505	1348.020239	19.018842
45.421598	1345.636781	19.023859
45.449785	1348.523076	19.028877
45.433589	1350.243906	19.033895
45.540881	1339.320498	19.038912
45.364402	1347.079963	19.043930
45.445709	1353.522754	19.048947
45.779165	1367.187457	19.053965
45.517463	1371.234335	19.058983
46.119891	1369.185079	19.064000
45.767092	1375.227719	19.069018
45.909020	1370.671288	19.074035
45.702809	1374.043636	19.079053
45.684590	1368.463346	19.084071
46.012594	1369.179958	19.089088
46.055528	1363.276164	19.094106
45.941795	1361.123052	19.099123
46.104666	1365.978748	19.104141
45.994323	1376.230386	19.109159
46.306829	1364.548977	19.114176
46.001410	1379.176546	19.119194
46.025136	1365.060708	19.124211
46.190333	1360.970499	19.129229
46.020302	1364.540787	19.134247
46.282384	1374.880362	19.139264
46.673702	1394.167702	19.144282
46.468043	1393.831356	19.149299
46.595083	1395.726896	19.154317
46.314200	1393.112488	19.159335
46.764881	1389.754518	19.164352
46.614920	1392.097885	19.169370
46.778487	1393.029911	19.174387
46.760821	1394.902955	19.179405
46.416967	1400.946486	19.184423
47.138234	1392.030012	19.189440
46.673431	1396.978623	19.194458
46.580591	1389.960309	19.199475
47.044571	1400.260959	19.204493
46.759936	1409.867471	19.209511
47.272846	1409.822376	19.214528
47.261135	1424.521433	19.219546
47.411340	1421.140375	19.224563
47.413234	1418.414574	19.229581
47.167946	1423.421727	19.234599
47.523428	1416.955539	19.239616
47.496853	1417.337955	19.244634
47.084805	1412.680327	19.249651
47.419609	1419.523293	19.254669
47.018361	1417.002431	19.259687
47.564422	1411.221215	19.264704
47.133121	1410.857664	19.269722
47.179930	1413.754273	19.274739
47.686346	1427.058898	19.279757
47.836709	1431.252914	19.284775
48.414205	1427.602288	19.289792
48.148024	1438.428582	19.294810
48.280095	1428.238795	19.299827
48.224132	1414.142013	19.304845
48.279857	1411.983671	19.309863
48.083230	1400.351497	19.314880
48.358759	1402.440559	19.319898
48.239131	1398.372698	19.324915
48.010605	1393.131154	19.329933
47.840666	1400.069103	19.334951
47.982642	1405.010553	19.339968
48.630149	1418.237480	19.344986
48.852162	1424.068034	19.350003
48.978272	1413.820190	19.355021
48.561012	1406.050871	19.360039
48.576543	1392.072584	19.365056
48.473038	1396.426341	19.370074
48.459671	1427.669144	19.375091
48.874968	1422.114691	19.380109
48.728348	1421.785498	19.385127
48.726491	1423.946475	19.390144
48.593579	1422.623686	19.395162
48.881382	1414.090779	19.400179
49.015842	1412.879623	19.405197
48.430900	1422.834288	19.410215
48.810510	1411.709837	19.415232
48.706282	1417.158192	19.420250
48.657148	1428.597745	19.425267
49.063154	1438.237950	19.430285
49.059212	1446.109445	19.435303
48.929407	1444.702282	19.440320
49.563408	1437.573834	19.445338
49.324137	1445.419728	19.450355
49.502162	1446.297002	19.455373
49.534820	1452.616396	19.460391
49.530947	1442.362890	19.465408
49.537949	1440.509458	19.470426
49.328254	1443.731217	19.475443
49.778742	1456.146320	19.480461
49.806374	1467.848385	19.485479
49.860817	1470.821693	19.490496
50.011012	1469.372890	19.495514
49.996257	1460.616435	19.500531
50.209524	1463.754780	19.505549
50.360911	1462.572707	19.510567
50.252695	1450.461689	19.515584
50.304377	1435.133298	19.520602
49.920160	1433.110001	19.525619
50.384307	1431.847798	19.530637
50.596069	1458.158959	19.535655
50.457616	1452.630043	19.540672
50.222871	1440.859270	19.545690
50.487624	1453.061820	19.550707
50.393059	1447.855950	19.555725
50.455186	1457.685781	19.560743
50.659025	1459.958767	19.565760
50.966945	1462.415699	19.570778
50.609483	1464.186354	19.575795
51.061477	1453.592401	19.580813
50.912656	1451.014383	19.585831
50.583655	1445.064663	19.590848
50.855638	1447.429906	19.595866
50.729459	1459.026331	19.600883
50.790111	1455.304191	19.605901
50.788531	1452.898641	19.610919
50.947445	1456.739678	19.615936
50.834966	1453.319824	19.620954
50.904721	1470.410528	19.625971
50.943147	1452.203241	19.630989
50.969326	1455.421381	19.636007
50.883806	1464.737480	19.641024
51.336181	1476.851503	19.646042
51.069073	1484.610689	19.651059
50.973100	1473.085022	19.656077
50.798382	1479.763563	19.661095
51.019300	1490.128929	19.666112
51.532555	1497.234899	19.671130
51.809409	1498.600926	19.676147
52.147590	1500.341836	19.681165
51.907095	1495.683730	19.686183
52.020545	1503.346055	19.691200
52.138157	1499.119202	19.696218
51.977004	1503.422691	19.701235
52.593769	1502.650958	19.706253
52.150299	1498.218977	19.711271
52.448569	1497.120061	19.716288
52.324835	1474.550263	19.721306
52.158062	1469.029180	19.726323
52.406528	1472.423114	19.731341
52.331993	1468.283989	19.736359
52.283398	1492.141492	19.741376
52.754905	1489.624927	19.746394
52.490613	1495.985239	19.751411
52.753952	1498.216489	19.756429
52.707091	1501.902240	19.761447
52.525393	1501.451688	19.766464
52.898550	1495.332931	19.771482
52.719459	1499.703563	19.776499
53.038457	1497.660277	19.781517
52.820700	1487.733885	19.786535
52.865638	1497.615013	19.791552
52.909960	1485.943273	19.796570
52.624290	1489.768561	19.801587
52.876428	1496.849657	19.806605
52.676514	1488.754547	19.811623
52.641886	1494.000462	19.816640
52.835666	1495.571975	19.821658
52.740378	1513.785715	19.826675
52.782908	1514.875977	19.831693
53.528085	1522.400248	19.836711
53.006118	1529.252842	19.841728
53.011325	1521.826897	19.846746
53.381031	1540.872725	19.851763
53.744440	1535.811861	19.856781
53.882115	1538.347781	19.861799
53.828654	1547.090121	19.866816
54.167918	1547.834798	19.871834
53.711551	1536.464819	19.876851
54.128465	1535.974992	19.881869
54.422242	1541.688986	19.886887
53.969377	1528.201121	19.891904
54.313694	1530.858336	19.896922
54.028549	1520.967096	19.901939
54.306078	1526.420389	19.906957
54.149012	1531.385411	19.911975
53.976206	1536.278237	19.916992
54.269095	1532.811325	19.922010
54.236492	1544.558067	19.927027
54.563809	1538.526805	19.932045
54.609974	1538.734188	19.937063
54.387195	1543.431355	19.942080
54.734985	1533.332947	19.947098
54.492221	1534.819265	19.952115
54.699624	1540.152680	19.957133
54.652801	1540.113257	19.962151
54.741539	1541.999803	19.967168
54.837247	1539.547423	19.972186
54.674463	1544.722843	19.977203
54.264431	1538.101467	19.982221
54.614220	1546.183734	19.987239
54.397192	1550.300426	19.992256
54.694373	1557.555587	19.997274
54.404661	1558.729604	20.002291
54.891898	1562.850162	20.007309
54.942752	1580.194115	20.012327
55.325587	1584.139446	20.017344
55.667599	1577.535659	20.022362
55.344130	1585.677453	20.027379
55.499580	1575.157716	20.032397
55.453313	1584.481168	20.037415
55.302231	1585.163730	20.042432
55.437411	1575.054435	20.047450
55.381383	1578.118102	20.052467
56.065343	1587.348600	20.057485
56.168948	1582.820500	20.062503
55.760061	1582.590633	20.067520
56.074294	1578.207187	20.072538
55.957192	1595.979361	20.077555
56.198409	1600.159168	20.082573
56.458636	1601.053155	20.087591
56.299553	1606.360660	20.092608
56.567779	1596.729714	20.097626
56.251548	1584.811694	20.102643
56.480108	1582.971166	20.107661
56.488732	1594.130806	20.112679
56.456292	1597.017343	20.117696
56.634559	1588.927280	20.122714
56.325357	1599.372226	20.127731
56.632497	1597.603332	20.132749
56.486476	1599.547260	20.137767
56.351495	1600.869282	20.142784
56.522595	1595.664256	20.147802
56.630935	1597.517642	20.152819
56.646629	1595.252911	20.157837
56.927972	1610.084723	20.162855
56.801808	1627.711977	20.167872
57.282914	1629.331205	20.172890
57.246941	1626.406913	20.177907
57.040502	1632.655339	20.182925
57.480052	1625.632231	20.187943
57.288163	1624.985331	20.192960
57.448130	1617.831354	20.197978
57.355490	1621.982981	20.202995
57.532350	1624.638017	20.208013
57.920614	1623.076948	20.213031
57.746068	1620.872058	20.218048
57.910118	1614.708745	20.223066
57.999542	1624.491249	20.228083
58.009005	1617.792113	20.233101
57.985416	1613.647663	20.238119
57.718003	1620.258935	20.243136
57.817832	1616.827908	20.248154
57.641794	1616.882714	20.253171
57.397327	1616.158693	20.258189
57.896418	1633.431639	20.263207
57.845964	1649.257797	20.268224
58.184038	1643.684164	20.273242
57.826186	1635.656466	20.278259
58.238429	1643.216632	20.283277
58.176082	1640.383319	20.288295
58.240559	1643.786889	20.293312
58.387573	1646.849627	20.298330
58.277726	1664.154535	20.303347
58.367361	1669.948046	20.308365
58.835387	1669.384399	20.313383
58.753988	1668.464084	20.318400
58.747306	1662.145555	20.323418
58.945951	1667.839520	20.328435
58.619192	1667.559832	20.333453
58.887960	1662.535070	20.338471
58.926192	1661.368962	20.343488
59.331624	1671.439725	20.348506
59.026503	1656.076099	20.353523
59.100531	1674.993097	20.358541
59.312192	1689.672744	20.363559
59.414487	1696.220865	20.368576
59.505182	1687.333041	20.373594
59.636949	1694.521561	20.378611
59.888264	1703.663527	20.383629
59.900650	1687.273278	20.388647
59.825427	1691.507867	20.393664
59.961852	1681.750660	20.398682
60.062619	1685.830516	20.403699
59.598247	1672.849550	20.408717
60.230156	1674.211924	20.413735
60.141941	1682.024265	20.418752
60.026581	1681.363903	20.423770
60.374051	1681.176123	20.428787
59.967466	1686.693533	20.433805
60.164865	1686.780996	20.438823
59.949682	1682.030847	20.443840
60.394944	1678.167020	20.448858
60.410830	1673.060109	20.453875
60.183769	1680.724965	20.458893
60.586591	1674.500046	20.463911
60.127519	1675.015496	20.468928
60.424826	1681.139195	20.473946
60.746464	1694.095906	20.478963
60.605008	1712.241931	20.483981
60.942509	1701.165585	20.488999
60.572730	1713.431671	20.494016
60.770867	1704.268172	20.499034
60.628696	1692.398808	20.504051
60.646908	1708.010113	20.509069
60.849447	1701.745116	20.514087
60.949208	1722.183116	20.519104
61.047041	1726.403234	20.524122
61.410509	1726.061623	20.529139
61.291707	1724.715605	20.534157
61.535347	1720.291052	20.539175
61.409606	1731.372643	20.544192
61.519701	1725.626096	20.549210
61.450389	1721.541551	20.554227
61.496876	1722.859127	20.559245
62.115097	1713.395358	20.564263
62.021808	1713.263628	20.569280
61.902234	1717.391393	20.574298
62.206861	1711.630752	20.579315
62.015506	1707.614055	20.584333
62.252177	1715.026555	20.589351
62.137063	1713.833865	20.594368
62.119191	1712.827437	20.599386
62.358878	1731.937550	20.604403
62.254627	1745.065214	20.609421
62.727838	1742.403052	20.614439
62.672074	1735.652066	20.619456
62.330816	1727.346373	20.624474
62.299977	1724.138928	20.629491
62.628263	1733.886282	20.634509
62.593566	1740.988605	20.639527
62.477088	1746.804461	20.644544
62.469618	1740.723435	20.649562
62.683159	1737.888518	20.654579
62.616410	1742.359909	20.659597
62.985648	1734.078700	20.664615
63.209708	1734.284978	20.669632
62.888777	1741.112645	20.674650
63.057103	1735.176136	20.679667
63.043790	1754.215174	20.684685
63.662861	1765.800246	20.689703
63.652899	1766.683861	20.694720
63.369703	1768.647372	20.699738
63.779267	1767.528830	20.704755
63.512651	1770.845121	20.709773
63.558600	1772.979334	20.714791
63.177939	1763.608089	20.719808
63.398567	1764.231475	20.724826
63.970673	1748.413452	20.729843
63.799354	1759.330562	20.734861
63.674652	1761.657991	20.739879
63.696244	1769.437233	20.744896
63.845756	1786.266259	20.749914
64.356683	1786.911660	20.754931
64.012611	1792.115210	20.759949
64.335297	1782.601512	20.764967
64.407694	1783.419129	20.769984
64.588027	1788.798451	20.775002
64.451940	1785.408417	20.780019
64.389553	1782.471146	20.785037
64.166848	1783.846685	20.790055
64.163540	1786.292208	20.795072
64.218568	1798.273848	20.800090
64.947426	1805.401746	20.805107
64.596452	1809.419028	20.810125
64.739546	1804.554007	20.815143
64.993868	1805.324574	20.820160
65.195692	1811.155863	20.825178
65.177246	1802.726208	20.830195
65.413616	1802.946591	20.835213
65.624838	1793.582840	20.840231
65.645530	1807.191843	20.845248
65.446859	1803.887759	20.850266
65.630037	1795.547559	20.855283
65.638539	1794.293844	20.860301
65.568919	1792.427465	20.865319
65.632754	1798.083563	20.870336
65.510933	1794.927781	20.875354
65.813544	1796.696663	20.880371
65.680010	1811.127671	20.885389
65.850512	1826.618210	20.890407
65.957904	1825.132367	20.895424
65.888164	1826.477858	20.900442
66.280023	1827.951648	20.905459
66.175196	1830.465169	20.910477
65.947972	1826.085478	20.915495
66.641734	1823.719860	20.920512
65.994710	1823.660127	20.925530
66.151177	1815.441664	20.930547
66.060547	1826.747434	20.935565
66.508514	1840.339659	20.940583
66.491650	1842.909091	20.945600
66.672835	1855.613599	20.950618
67.021680	1850.812136	20.955635
66.776835	1849.841311	20.960653
66.663393	1855.997655	20.965671
66.821828	1848.148146	20.970688
66.660308	1850.594678	20.975706
66.832530	1846.416564	20.980723
66.913128	1857.935742	20.985741
67.038078	1871.792898	20.990759
67.291420	1874.849889	20.995776
67.235342	1890.104380	21.000794
67.323427	1880.711751	21.005811
67.462827	1874.589032	21.010829
67.315558	1874.261903	21.015847
67.709798	1869.901351	21.020864
67.787502	1873.364987	21.025882
67.820612	1862.736963	21.030899
67.962878	1864.394604	21.035917
67.805491	1867.436133	21.040935
68.339907	1862.813000	21.045952
68.229040	1870.488632	21.050970
67.926407	1870.628967	21.055987
68.208077	1880.210114	21.061005
68.045255	1880.321788	21.066023
68.614858	1877.410176	21.071040
68.600923	1878.891710	21.076058
68.610477	1878.276406	21.081075
68.498933	1883.947400	21.086093
68.504174	1878.702024	21.091111
69.043909	1877.985551	21.096128
68.572374	1876.935327	21.101146
68.908602	1874.348975	21.106163
68.868578	1875.804512	21.111181
68.793640	1880.877702	21.116199
68.808228	1878.217436	21.121216
68.656444	1874.840611	21.126234
69.061497	1886.318688	21.131251
68.724568	1896.155027	21.136269
69.089332	1913.014300	21.141287
69.084105	1914.539278	21.146304
69.010750	1927.899781	21.151322
69.248854	1906.520649	21.156339
69.547805	1925.328269	21.161357
69.597744	1926.046067	21.166375
69.870895	1927.963152	21.171392
69.819043	1937.450736	21.176410
70.118512	1933.466889	21.181427
70.217420	1937.661689	21.186445
69.947622	1926.962906	21.191463
70.199486	1928.279567	21.196480
69.925588	1935.118034	21.201498
70.621692	1928.273184	21.206515
70.513308	1922.614709	21.211533
70.370420	1924.099093	21.216551
70.524019	1920.709885	21.221568
70.554114	1922.465634	21.226586
70.271567	1919.759675	21.231603
70.595909	1922.268295	21.236621
70.408288	1920.237184	21.241639
70.579417	1932.552467	21.246656
70.442372	1952.936277	21.251674
70.890869	1944.211904	21.256691
70.958054	1951.973846	21.261709
70.983626	1959.465511	21.266727
70.948323	1953.767758	21.271744
70.780662	1962.003638	21.276762
70.888076	1965.592300	21.281779
71.278575	1977.279945	21.286797
71.274048	1980.295005	21.291815
71.254774	1975.511541	21.296832
71.701638	1982.182657	21.301850
71.435592	1973.930916	21.306867
71.471610	1978.515282	21.311885
71.467833	1980.394366	21.316903
71.873168	1976.143761	21.321920
71.839713	1995.238398	21.326938
71.947796	1998.771050	21.331955
72.549452	2001.225107	21.336973
72.191492	2009.422439	21.341991
72.408941	1997.653932	21.347008
72.390916	2008.841117	21.352026
72.725028	1994.479610	21.357043
72.912926	1983.625871	21.362061
72.468608	1973.219343	21.367079
72.375702	1960.695932	21.372096
72.538176	1977.675779	21.377114
72.384260	1980.396275	21.382131
72.832845	1993.715693	21.387149
72.762478	1997.442461	21.392167
72.661354	1993.222950	21.397184
72.952916	1997.237440	21.402202
72.781593	1995.229605	21.407219
73.108947	1991.588379	21.412237
73.161779	2012.644389	21.417255
73.291598	2018.495159	21.422272
72.632684	2019.503560	21.427290
73.182616	2017.392838	21.432307
73.513625	2016.827064	21.437325
73.504434	2021.327981	21.442343
73.874467	2011.079909	21.447360
74.116008	2014.966856	21.452378
73.921806	2014.286855	21.457395
74.202614	2009.559603	21.462413
74.159807	2015.867311	21.467431
74.260852	2011.883620	21.472448
73.946801	2009.690748	21.477466
74.297632	2010.355187	21.482483
74.170865	2027.282976	21.487501
74.464173	2031.367660	21.492519
74.801006	2037.932213	21.497536
74.881244	2041.549409	21.502554
74.675854	2039.797609	21.507571
74.927625	2038.872896	21.512589
74.793096	2039.009808	21.517607
74.937792	2035.080696	21.522624
74.791750	2036.712074	21.527642
74.794950	2044.927188	21.532659
75.074441	2030.075466	21.537677
74.819000	2043.388655	21.542695
74.891734	2040.032889	21.547712
74.987694	2036.576819	21.552730
75.152811	2039.987042	21.557747
75.132380	2049.236021	21.562765
75.491371	2064.177858	21.567783
75.654103	2059.558333	21.572800
75.200023	2058.190235	21.577818
75.598466	2062.162242	21.582835
75.624026	2059.945811	21.587853
75.302899	2067.990221	21.592871
75.627913	2086.563400	21.597888
76.095094	2082.567102	21.602906
76.129764	2087.281650	21.607923
76.515804	2084.370472	21.612941
76.282936	2080.384567	21.617959
76.362523	2075.898491	21.622976
76.350124	2075.370676	21.627994
76.133823	2081.533115	21.633011
76.156097	2079.031390	21.638029
76.168677	2097.756316	21.643047
76.747510	2096.853041	21.648064
76.930100	2107.764555	21.653082
76.898226	2113.296058	21.658099
77.179153	2102.812278	21.663117
76.761523	2112.882594	21.668135
77.069632	2106.352311	21.673152
77.147628	2106.191429	21.678170
76.964291	2106.748641	21.683187
77.180802	2104.065928	21.688205
77.102085	2102.737649	21.693223
77.066360	2094.326444	21.698240
77.068949	2116.227947	21.703258
76.783641	2132.201753	21.708275
77.289051	2132.971318	21.713293
77.114698	2148.467306	21.718311
77.747828	2157.490024	21.723328
78.159175	2156.276276	21.728346
78.169214	2161.625261	21.733363
78.506344	2157.701660	21.738381
78.754290	2158.912687	21.743399
78.619070	2155.468095	21.748416
78.911933	2158.804042	21.753434
78.495670	2142.711063	21.758451
78.617454	2129.638566	21.763469
78.778644	2149.849629	21.768487
78.770611	2138.719156	21.773504
78.928051	2140.686531	21.778522
78.698431	2141.185656	21.783539
79.180704	2150.860928	21.788557
78.781150	2150.920457	21.793575
78.734549	2142.400787	21.798592
78.814821	2140.546164	21.803610
79.030680	2149.382839	21.808627
79.144641	2141.943709	21.813645
79.052623	2145.773314	21.818663
79.490400	2167.361882	21.823680
79.545708	2172.549039	21.828698
79.183867	2186.444553	21.833715
79.492486	2178.351501	21.838733
79.286249	2182.179553	21.843751
79.436700	2178.308509	21.848768
79.435015	2193.605869	21.853786
79.709592	2210.454413	21.858803
79.933638	2201.784384	21.863821
79.824128	2203.405399	21.868839
80.127083	2211.392618	21.873856
80.441853	2218.543601	21.878874
80.529922	2230.398445	21.883891
80.692393	2224.906046	21.888909
80.689706	2235.501856	21.893927
80.830237	2226.565708	21.898944
81.338840	2217.730441	21.903962
81.167686	2216.408795	21.908979
81.705431	2207.763204	21.913997
81.338308	2188.344200	21.919015
81.331695	2185.268873	21.924032
81.409055	2166.136552	21.929050
81.192634	2186.189704	21.934067
81.095150	2173.575536	21.939085
81.222257	2178.280319	21.944103
81.218058	2193.559590	21.949120
81.336031	2199.662006	21.954138
81.363424	2216.201864	21.959155
81.617279	2211.975096	21.964173
81.461668	2211.509177	21.969191
81.199247	2220.868012	21.974208
81.896981	2228.051658	21.979226
81.491093	2235.466068	21.984243
81.904541	2232.836951	21.989261
81.599982	2240.483414	21.994279
81.420655	2242.932955	21.999296
81.810158	2263.344563	22.004314
81.903132	2270.000774	22.009331
82.236844	2255.635944	22.014349
82.644181	2270.243978	22.019367
82.571668	2285.669302	22.024384
82.873579	2287.589546	22.029402
82.932175	2289.869774	22.034419
83.081584	2278.968656	22.039437
83.484742	2284.758128	22.044455
83.391330	2286.708391	22.049472
83.682195	2276.815788	22.054490
83.557278	2276.256199	22.059507
83.744633	2261.615189	22.064525
83.782268	2251.632240	22.069543
83.404510	2247.362788	22.074560
83.823811	2248.791918	22.079578
83.750343	2262.472819	22.084595
84.088722	2260.183305	22.089613
84.018479	2254.463666	22.094631
83.854683	2267.511862	22.099648
84.614289	2262.954090	22.104666
84.246054	2276.314106	22.109683
84.368407	2270.679901	22.114701
84.286902	2270.379278	22.119719
83.883346	2272.656884	22.124736
84.576965	2261.049901	22.129754
84.281466	2269.796105	22.134771
84.524660	2267.852679	22.139789
84.363776	2266.279712	22.144807
84.164295	2271.985091	22.149824
84.885416	2284.267863	22.154842
84.766046	2303.375529	22.159859
84.767548	2293.906432	22.164877
84.784341	2299.231904	22.169895
84.683686	2313.111847	22.174912
85.035608	2319.016512	22.179930
85.124260	2335.416034	22.184947
84.999052	2328.914881	22.189965
85.157213	2328.203691	22.194983
85.226856	2353.624508	22.200000
85.633347	2349.108640	22.205018
85.689394	2360.676353	22.210035
85.889817	2350.325033	22.215053
86.075670	2353.596847	22.220071
86.093959	2356.815299	22.225088
86.374153	2352.250259	22.230106
86.375536	2350.777194	22.235123
86.273492	2362.454552	22.240141
86.909145	2372.971145	22.245159
86.775339	2382.527690	22.250176
86.541372	2369.497751	22.255194
86.564686	2381.214606	22.260211
86.648378	2370.834566	22.265229
86.775599	2370.905701	22.270247
86.552397	2368.524497	22.275264
86.892644	2368.995816	22.280282
86.868526	2373.300872	22.285299
87.147562	2381.020866	22.290317
87.134384	2387.412799	22.295335
87.372142	2403.123105	22.300352
87.779866	2388.132877	22.305370
87.635645	2393.369286	22.310387
87.728626	2399.700732	22.315405
87.952929	2384.276286	22.320423
87.707253	2394.089954	22.325440
88.042532	2387.896411	22.330458
88.031960	2386.671397	22.335475
88.000063	2375.966380	22.340493
88.023819	2375.687305	22.345511
87.936239	2386.503976	22.350528
88.193658	2398.904167	22.355546
88.361057	2408.286836	22.360563
88.171737	2420.761797	22.365581
88.590304	2412.793341	22.370599
88.221682	2420.026461	22.375616
88.504812	2417.080291	22.380634
88.625947	2436.583755	22.385651
88.665852	2442.144832	22.390669
88.995028	2438.180745	22.395687
88.581690	2452.231485	22.400704
88.975996	2439.870341	22.405722
89.030917	2456.655516	22.410739
88.891358	2471.255071	22.415757
89.273200	2462.785556	22.420775
89.529178	2470.673201	22.425792
89.731274	2463.856368	22.430810
89.741563	2468.669168	22.435827
89.682121	2478.324094	22.440845
90.081267	2489.896124	22.445863
89.980374	2498.391325	22.450880
90.187578	2496.117985	22.455898
90.658394	2500.073399	22.460915
90.661652	2494.802552	22.465933
90.627642	2482.671353	22.470951
90.552375	2495.565704	22.475968
90.943339	2484.127178	22.480986
90.725972	2494.907929	22.486003
90.873682	2496.322205	22.491021
91.116093	2481.223423	22.496039
91.120681	2494.514024	22.501056
91.123943	2483.495614	22.506074
91.441635	2483.061565	22.511091
90.951938	2478.488517	22.516109
91.298562	2484.784697	22.521127
91.397679	2485.810932	22.526144
90.949410	2490.408699	22.531162
91.496506	2503.213007	22.536179
91.315452	2503.796626	22.541197
91.600372	2501.494668	22.546215
91.580977	2513.319487	22.551232
92.002831	2528.298612	22.556250
92.185374	2532.128525	22.561267
92.396207	2538.716910	22.566285
92.669583	2536.203461	22.571303
92.364838	2550.324110	22.576320
92.479182	2541.201162	22.581338
92.504068	2542.401118	22.586355
92.451101	2533.788975	22.591373
92.881237	2526.811124	22.596391
92.679091	2540.368288	22.601408
92.382990	2533.257905	22.606426
92.647389	2553.437837	22.611443
92.673234	2562.755447	22.616461
93.053542	2559.493143	22.621479
92.687025	2577.241979	22.626496
93.141877	2584.658933	22.631514
93.541054	2589.338875	22.636531
93.283493	2594.017702	22.641549
93.662572	2590.865444	22.646567
93.461064	2597.711900	22.651584
93.661728	2591.954371	22.656602
94.196275	2599.061662	22.661619
93.784136	2603.938143	22.666637
94.170091	2603.927857	22.671655
94.102822	2615.868167	22.676672
94.452460	2609.152442	22.681690
94.647923	2606.970799	22.686707
94.286226	2605.446794	22.691725
94.777086	2601.382269	22.696743
94.783002	2602.453473	22.701760
94.693281	2601.832135	22.706778
94.955786	2604.470012	22.711795
94.774337	2604.689504	22.716813
95.092573	2594.509081	22.721831
94.735659	2607.430076	22.726848
94.890103	2622.894145	22.731866
95.171484	2620.539997	22.736883
95.048131	2627.966084	22.741901
95.265886	2622.796697	22.746919
95.403570	2639.247480	22.751936
95.128219	2656.202520	22.756954
95.551488	2650.068721	22.761971
95.565243	2658.722992	22.766989
95.760157	2662.957609	22.772007
95.815400	2691.381563	22.777024
95.962683	2693.768829	22.782042
96.116407	2691.660625	22.787059
96.215716	2694.792500	22.792077
96.425865	2684.560224	22.797095
96.195872	2693.563159	22.802112
96.675225	2715.238133	22.807130
96.781777	2708.672462	22.812147
96.539672	2709.388253	22.817165
97.383946	2704.088335	22.822183
97.255194	2711.716157	22.827200
97.309439	2710.387466	22.832218
97.269138	2706.669537	22.837235
97.075765	2716.497977	22.842253
97.510269	2727.166236	22.847271
97.805339	2730.080260	22.852288
97.958496	2733.779645	22.857306
98.144277	2732.713447	22.862323
98.071719	2740.700903	22.867341
98.483090	2734.579672	22.872359
98.262889	2736.240724	22.877376
98.270391	2727.092047	22.882394
98.394967	2720.975388	22.887411
98.251063	2730.822813	22.892429
98.547707	2722.101104	22.897447
98.965767	2727.064203	22.902464
98.496685	2726.635993	22.907482
98.918527	2719.805503	22.912499
98.535453	2726.887996	22.917517
98.760661	2730.052974	22.922535
98.960543	2745.749424	22.927552
99.166631	2751.723680	22.932570
99.216528	2741.829339	22.937587
99.167393	2752.453665	22.942605
99.288204	2742.949579	22.947623
99.654856	2762.474619	22.952640
99.425094	2774.791586	22.957658
99.666604	2780.057574	22.962675
99.612594	2785.305558	22.967693
100.102407	2778.066516	22.972711
100.243164	2776.468359	22.977728
100.174902	2768.374799	22.982746
100.658586	2768.509368	22.987763
100.520721	2771.755335	22.992781
100.198907	2763.382866	22.997799
100.461881	2776.808893	23.002816
100.344628	2785.355388	23.007834
100.913295	2788.174909	23.012851
100.788247	2807.576280	23.017869
101.090637	2793.983917	23.022887
101.151869	2799.776648	23.027904
100.644220	2793.487449	23.032922
101.348037	2787.749701	23.037939
100.951772	2800.134809	23.042957
101.434987	2802.738148	23.047975
101.335623	2822.465232	23.052992
101.527281	2824.305366	23.058010
101.684987	2821.275942	23.063027
101.672111	2820.988749	23.068045
101.561794	2814.080959	23.073063
102.230002	2819.867699	23.078080
102.159820	2846.268056	23.083098
102.370671	2840.564265	23.088115
102.202385	2846.351703	23.093133
102.369608	2845.335818	23.098151
102.571885	2840.818579	23.103168
102.531035	2849.416244	23.108186
103.009737	2829.192565	23.113203
102.751674	2841.630815	23.118221
103.039855	2850.528757	23.123239
103.218485	2857.914011	23.128256
103.350271	2865.924790	23.133274
103.402744	2867.761987	23.138291
103.316858	2863.717289	23.143309
103.366700	2860.447427	23.148327
103.384339	2863.378667	23.153344
103.395619	2868.286709	23.158362
103.696384	2882.368041	23.163379
103.916618	2884.147542	23.168397
103.608089	2892.646229	23.173415
104.032268	2887.079557	23.178432
103.866806	2894.806467	23.183450
104.354526	2913.888389	23.188467
104.345827	2914.609642	23.193485
104.331154	2920.553973	23.198503
104.487505	2910.649775	23.203520
104.491849	2916.814596	23.208538
104.659771	2936.916110	23.213555
104.938473	2943.591077	23.218573
105.102377	2942.982069	23.223591
105.376065	2938.749855	23.228608
105.299856	2944.607918	23.233626
105.276729	2941.984033	23.238643
105.368370	2950.203488	23.243661
105.723352	2961.747353	23.248679
105.794324	2965.229673	23.253696
105.954717	2962.282855	23.258714
106.234720	2963.481948	23.263731
106.115433	2962.502466	23.268749
106.580868	2955.694976	23.273767
106.451749	2964.187622	23.278784
106.537342	2957.322142	23.283802
106.868807	2954.569856	23.288819
106.723620	2952.631195	23.293837
106.622023	2959.625060	23.298855
106.964782	2950.131351	23.303872
106.692472	2967.236237	23.308890
107.055635	2978.194458	23.313907
107.144748	2978.279781	23.318925
107.097187	2988.748481	23.323943
107.437782	2980.141017	23.328960
107.236046	2982.841647	23.333978
107.823613	2979.394537	23.338995
107.511334	2984.151442	23.344013
107.452560	2988.158836	23.349031
107.815968	2996.994009	23.354048
107.487517	3013.331400	23.359066
107.860112	3008.885530	23.364083
108.036720	3010.247821	23.369101
108.192293	3011.258445	23.374119
108.208340	3016.921324	23.379136
108.358489	3039.070977	23.384154
108.688101	3031.634307	23.389171
108.852504	3035.059437	23.394189
109.012770	3035.978333	23.399207
108.847747	3027.400218	23.404224
108.790909	3021.293791	23.409242
108.860106	3028.264922	23.414259
109.299226	3041.080466	23.419277
109.221741	3047.273455	23.424295
109.594788	3053.155219	23.429312
109.549122	3065.856540	23.434330
109.876485	3054.332845	23.439347
109.679371	3045.559622	23.444365
109.706036	3060.817702	23.449383
109.593807	3060.148493	23.454400
109.754103	3083.518296	23.459418
109.802193	3079.875021	23.464435
110.134875	3076.883908	23.469453
110.502236	3095.372144	23.474471
110.876843	3098.257321	23.479488
110.516420	3109.585851	23.484506
110.723588	3109.000780	23.489523
111.040175	3096.418501	23.494541
110.745976	3104.402676	23.499559
111.304921	3095.683007	23.504576
111.241737	3113.230639	23.509594
111.580744	3117.411207	23.514611
111.668573	3122.955537	23.519629
111.291764	3126.564002	23.524647
111.868172	3118.191069	23.529664
111.980046	3117.933616	23.534682
112.098159	3116.041508	23.539699
112.127563	3114.069590	23.544717
111.940977	3129.383125	23.549735
111.991046	3142.683678	23.554752
112.183172	3139.366577	23.559770
112.304346	3145.119982	23.564787
112.353348	3152.860729	23.569805
112.258802	3161.927737	23.574823
112.739784	3172.432294	23.579840
112.602497	3173.670567	23.584858
112.471029	3175.187432	23.589875
113.034634	3186.377601	23.594893
112.976076	3195.638297	23.599911
113.366327	3197.322356	23.604928
113.359732	3203.151666	23.609946
113.746599	3221.770694	23.614963
114.183960	3230.570526	23.619981
113.948496	3235.384088	23.624999
114.336843	3229.266872	23.630016
114.176443	3229.788823	23.635034
114.506727	3235.549377	23.640051
114.596661	3228.494064	23.645069
114.541990	3223.886959	23.650087
114.739468	3220.282312	23.655104
114.885806	3216.468787	23.660122
114.980338	3221.591527	23.665139
115.123236	3218.682601	23.670157
114.978222	3221.417192	23.675175
114.965243	3223.039654	23.680192
115.214336	3230.411451	23.685210
115.204056	3239.749621	23.690227
115.439496	3242.443277	23.695245
115.575435	3243.218954	23.700263
115.786581	3238.530037	23.705280
115.720893	3245.190097	23.710298
115.782241	3243.479437	23.715315
115.897744	3244.109663	23.720333
115.601682	3256.020618	23.725351
116.041056	3254.439123	23.730368
115.715677	3264.982353	23.735386
115.921797	3279.873106	23.740403
116.326403	3287.258557	23.745421
116.380203	3297.302765	23.750439
116.689897	3303.636106	23.755456
117.116605	3308.805070	23.760474
117.190919	3323.982283	23.765491
117.438785	3315.669546	23.770509
117.203013	3323.496112	23.775527
117.549434	3315.344243	23.780544
117.495449	3320.547122	23.785562
117.445709	3322.507606	23.790579
117.919083	3325.894641	23.795597
118.224454	3342.450702	23.800615
118.629915	3333.393281	23.805632
118.564477	3346.214257	23.810650
118.349177	3337.857312	23.815667
118.803372	3336.484796	23.820685
118.542502	3339.101172	23.825703
118.566931	3344.189884	23.830720
118.793392	3343.104311	23.835738
118.697616	3350.840382	23.840755
118.971108	3345.662319	23.845773
119.190631	3340.412868	23.850791
119.078169	3357.794898	23.855808
119.223931	3360.284106	23.860826
119.089436	3364.145847	23.865843
119.314463	3363.000267	23.870861
119.072250	3381.539760	23.875879
119.286612	3377.727140	23.880896
119.824601	3392.187423	23.885914
119.661713	3412.584110	23.890931
120.227546	3411.501408	23.895949
120.353958	3426.079869	23.900967
120.797060	3409.614530	23.905984
120.845555	3417.169643	23.911002
120.849260	3416.805277	23.916019
121.016432	3411.426264	23.921037
120.975037	3410.314553	23.926055
121.453461	3423.774769	23.931072
121.309344	3427.214841	23.936090
121.681171	3438.655080	23.941107
121.546661	3433.442556	23.946125
121.671086	3440.663025	23.951143
121.402688	3434.415851	23.956160
121.851142	3438.403957	23.961178
121.616046	3432.274513	23.966195
121.920734	3438.387847	23.971213
121.958738	3457.690973	23.976231
121.874815	3462.461796	23.981248
122.081371	3466.335609	23.986266
121.835086	3478.911800	23.991283
122.669540	3480.545580	23.996301
122.288729	3489.064825	24.001319
122.444013	3496.115624	24.006336
122.820564	3504.232683	24.011354
123.251334	3517.151196	24.016371
123.257022	3517.453115	24.021389
123.260231	3519.914369	24.026407
123.570147	3512.847708	24.031424
123.671239	3506.443651	24.036442
123.745843	3514.007483	24.041459
124.287022	3532.111118	24.046477
124.286307	3538.604228	24.051495
124.451906	3540.559013	24.056512
124.517391	3535.136944	24.061530
124.233304	3538.294270	24.066547
124.881852	3531.248711	24.071565
124.322892	3531.276746	24.076583
124.832051	3533.443975	24.081600
124.896771	3529.659243	24.086618
124.922591	3524.824525	24.091635
125.100709	3521.533288	24.096653
125.190393	3533.532182	24.101671
125.366882	3547.070056	24.106688
125.323870	3552.872844	24.111706
125.420777	3555.682415	24.116723
125.575327	3547.896880	24.121741
125.258893	3570.706103	24.126759
125.599585	3580.513995	24.131776
125.688491	3572.790897	24.136794
125.850233	3595.589896	24.141811
126.365348	3598.790138	24.146829
126.758642	3607.557712	24.151847
126.424033	3605.889336	24.156864
126.597992	3604.595875	24.161882
126.657459	3622.810868	24.166899
127.163295	3624.438434	24.171917
127.454446	3632.412198	24.176935
127.568965	3630.238305	24.181952
127.871145	3631.872026	24.186970
127.397349	3626.976666	24.191987
127.673761	3625.213428	24.197005
127.605792	3621.125010	24.202023
128.209588	3631.328408	24.207040
128.039848	3640.237253	24.212058
128.275129	3647.984811	24.217075
128.592068	3641.938716	24.222093
128.512647	3644.351063	24.227111
128.191392	3645.897425	24.232128
128.622566	3649.610852	24.237146
128.874525	3664.956255	24.242163
128.844861	3668.244736	24.247181
129.239311	3675.906894	24.252199
128.760082	3671.580211	24.257216
129.283235	3676.815233	24.262234
129.473027	3701.314298	24.267251
129.570169	3697.391070	24.272269
129.480539	3701.708913	24.277287
129.644080	3708.386344	24.282304
129.877264	3705.592714	24.287322
129.886549	3734.747925	24.292339
130.020257	3737.964879	24.297357
130.038908	3731.866938	24.302375
130.012099	3736.413793	24.307392
130.701214	3739.095821	24.312410
130.702131	3746.306167	24.317427
130.942121	3744.532014	24.322445
131.109276	3752.596064	24.327463
130.598397	3761.752427	24.332480
131.030217	3764.175834	24.337498
131.204023	3778.756228	24.342515
131.311862	3785.909121	24.347533
131.559256	3796.053507	24.352551
132.008321	3794.849544	24.357568
131.922336	3804.493145	24.362586
132.112906	3800.057110	24.367603
131.980961	3808.175431	24.372621
132.256334	3807.201038	24.377639
132.235778	3813.441212	24.382656
132.394804	3823.293902	24.387674
132.596972	3835.909535	24.392691
132.936869	3828.277060	24.397709
132.924659	3827.135680	24.402727
133.219723	3828.238242	24.407744
133.747926	3835.576718	24.412762
133.732913	3841.713608	24.417779
134.044675	3834.910709	24.422797
134.043250	3846.787506	24.427815
134.270404	3841.811074	24.432832
134.621998	3830.821459	24.437850
134.457562	3817.962285	24.442867
134.410056	3810.946395	24.447885
134.451311	3813.680963	24.452903
134.417255	3830.802471	24.457920
134.766448	3831.586579	24.462938
134.738410	3835.440654	24.467955
134.871079	3827.154201	24.472973
134.665118	3836.845248	24.477991
135.016368	3850.788766	24.483008
135.207346	3855.633111	24.488026
135.241249	3867.592277	24.493043
135.431755	3856.239100	24.498061
135.458138	3867.307257	24.503079
135.746038	3889.482168	24.508096
136.200162	3881.906751	24.513114
135.803348	3896.118272	24.518131
136.208387	3895.740214	24.523149
135.952801	3906.742466	24.528167
136.436955	3919.564274	24.533184
136.836917	3918.266449	24.538202
137.138268	3931.074430	24.543219
136.537638	3925.088785	24.548237
137.028678	3931.788088	24.553255
136.883534	3943.785617	24.558272
137.253371	3942.179345	24.563290
137.123794	3944.791014	24.568307
137.433301	3957.848099	24.573325
137.850789	3969.408354	24.578343
137.964781	3973.309038	24.583360
138.083922	3966.693900	24.588378
138.032259	3977.941223	24.593395
138.163570	3996.607425	24.598413
138.562899	3991.167336	24.603431
138.801342	4002.284745	24.608448
138.632604	3997.054467	24.613466
138.897264	4000.200969	24.618483
138.682798	4014.154419	24.623501
139.092727	4028.557351	24.628519
139.105270	4038.097762	24.633536
139.182697	4031.981705	24.638554
139.479943	4056.282800	24.643571
139.519790	4063.865646	24.648589
139.959254	4058.571669	24.653607
139.876618	4055.954299	24.658624
140.246741	4067.647685	24.663642
140.384583	4085.196988	24.668659
140.510054	4078.090128	24.673677
140.873123	4083.559305	24.678695
140.746439	4088.802431	24.683712
140.733483	4076.346774	24.688730
140.698086	4085.604554	24.693747
141.286989	4098.820258	24.698765
141.377656	4097.535822	24.703783
141.570801	4104.371934	24.708800
141.696172	4091.833512	24.713818
141.602358	4101.683742	24.718835
141.562550	4103.583615	24.723853
141.877640	4107.237620	24.728871
141.584054	4133.199891	24.733888
141.758497	4130.717928	24.738906
142.159897	4134.757715	24.743923
142.464898	4151.466689	24.748941
142.643070	4154.344818	24.753959
142.567872	4155.295283	24.758976
142.658029	4154.784282	24.763994
142.895940	4169.908061	24.769011
143.102933	4179.860533	24.774029
143.345700	4176.138705	24.779047
143.408156	4186.645118	24.784064
143.543783	4181.066702	24.789082
144.121105	4199.238765	24.794099
144.154333	4208.074952	24.799117
144.673466	4195.859511	24.804135
144.511609	4204.607501	24.809152
144.461068	4195.163194	24.814170
144.652190	4197.572181	24.819187
144.765579	4195.531883	24.824205
145.182256	4184.734431	24.829223
144.956234	4197.355880	24.834240
145.149617	4208.306851	24.839258
145.342276	4218.438916	24.844275
145.379889	4225.580405	24.849293
145.323478	4227.263319	24.854311
145.190273	4233.447887	24.859328
145.399599	4241.145305	24.864346
145.798827	4253.596345	24.869363
145.750969	4274.234600	24.874381
146.198243	4276.120795	24.879399
146.138930	4283.318521	24.884416
146.356554	4291.371343	24.889434
146.293657	4295.541591	24.894451
147.007644	4311.223807	24.899469
147.400954	4309.990056	24.904487
146.936188	4322.602303	24.909504
147.760005	4331.606938	24.914522
148.008283	4334.226208	24.919539
147.958325	4341.290104	24.924557
148.135965	4332.536412	24.929575
148.195835	4333.720476	24.934592
148.018534	4332.993073	24.939610
148.105470	4331.462737	24.944627
148.131921	4338.283234	24.949645
148.582609	4351.441706	24.954663
148.682396	4356.451330	24.959680
148.697158	4356.089048	24.964698
148.878331	4362.728008	24.969715
148.856518	4390.337346	24.974733
148.832759	4393.130031	24.979751
149.002456	4398.647872	24.984768
149.250718	4419.644453	24.989786
149.302458	4414.316105	24.994803
149.622793	4430.629855	24.999821
150.156594	4438.659548	25.004839
150.100818	4449.273129	25.009856
150.524004	4453.685839	25.014874
150.808407	4437.957247	25.019891
150.693304	4447.504076	25.024909
151.042039	4446.323373	25.029927
151.040304	4457.073707	25.034944
151.193233	4466.777786	25.039962
151.487509	4472.475065	25.044979
151.943457	4467.783847	25.049997
151.746455	4468.656053	25.055015
151.794588	4455.870237	25.060032
151.759424	4457.592974	25.065050
151.957591	4457.157800	25.070067
151.798454	4462.892338	25.075085
152.164360	4485.643082	25.080103
152.490653	4494.053678	25.085120
152.012494	4495.662321	25.090138
152.292650	4505.362687	25.095155
152.586844	4514.856760	25.100173
152.781115	4517.772456	25.105191
153.055902	4529.385892	25.110208
153.233869	4549.027887	25.115226
153.308558	4545.314897	25.120243
153.502253	4554.371217	25.125261
153.324670	4554.062825	25.130279
153.569932	4575.464912	25.135296
153.668009	4580.676504	25.140314
154.464060	4582.971228	25.145331
154.406004	4593.685302	25.150349
154.663211	4600.663811	25.155367
154.764067	4600.069119	25.160384
154.927803	4597.552630	25.165402
155.137491	4601.529772	25.170419
154.934471	4617.898070	25.175437
155.353647	4606.542330	25.180455
155.714872	4611.663903	25.185472
155.686321	4612.779934	25.190490
155.904623	4629.399027	25.195507
155.984591	4645.293651	25.200525
156.252500	4641.644732	25.205543
156.204151	4641.799290	25.210560
156.467690	4657.219355	25.215578
156.950466	4658.019197	25.220595
157.001878	4669.149143	25.225613
157.345511	4670.771389	25.230631
157.071459	4663.267324	25.235648
156.869864	4668.696306	25.240666
157.637763	4681.594627	25.245683
157.150047	4697.660466	25.250701
157.222948	4695.700837	25.255719
157.423166	4710.839255	25.260736
157.736665	4715.671853	25.265754
158.209702	4718.945455	25.270771
158.259640	4735.661051	25.275789
158.682421	4753.964090	25.280807
158.592840	4743.822625	25.285824
158.218716	4754.374918	25.290842
158.727604	4769.555224	25.295859
159.027461	4780.221197	25.300877
159.197436	4774.642399	25.305895
159.546257	4792.185917	25.310912
159.834176	4808.016352	25.315930
160.096974	4798.237861	25.320947
160.019550	4806.697348	25.325965
159.872863	4810.153108	25.330983
160.550064	4810.648276	25.336000
160.609204	4839.752393	25.341018
160.787405	4820.275662	25.346035
160.839649	4836.052996	25.351053
161.111558	4826.993600	25.356071
161.099042	4824.717320	25.361088
160.919173	4857.062482	25.366106
161.510944	4863.487193	25.371123
161.264063	4870.021606	25.376141
161.573033	4879.811942	25.381159
162.045776	4888.175666	25.386176
161.836030	4888.230934	25.391194
161.970759	4892.014218	25.396211
161.976732	4897.790097	25.401229
162.375934	4907.629305	25.406247
162.691700	4921.807654	25.411264
162.871461	4930.769627	25.416282
162.801896	4918.384105	25.421299
162.954306	4940.381710	25.426317
163.309574	4948.808231	25.431335
163.721857	4948.408479	25.436352
163.490658	4946.175473	25.441370
163.632618	4958.794103	25.446387
163.572465	4977.627843	25.451405
163.720398	4980.397721	25.456423
163.962143	4983.057561	25.461440
163.864470	5003.684542	25.466458
164.472021	4996.907784	25.471475
164.644002	5015.586579	25.476493
164.663108	5033.539359	25.481511
165.106836	5032.258618	25.486528
165.284792	5041.724212	25.491546
165.558826	5050.201253	25.496563
165.574834	5054.498039	25.501581
165.837441	5052.680227	25.506599
166.114479	5062.353102	25.511616
166.132566	5084.883495	25.516634
166.161706	5081.888314	25.521651
166.154122	5075.809553	25.526669
166.855613	5090.128968	25.531687
167.070705	5099.664844	25.536704
167.175267	5098.255166	25.541722
167.555750	5094.184269	25.546739
167.475662	5107.474564	25.551757
167.739641	5101.988774	25.556775
167.841191	5107.535474	25.561792
167.974204	5126.054673	25.566810
168.364515	5129.598808	25.571827
168.240486	5131.426901	25.576845
168.330843	5129.836066	25.581863
168.513824	5132.971119	25.586880
168.604107	5160.219865	25.591898
168.687611	5154.170886	25.596915
168.836539	5160.706050	25.601933
168.976168	5172.075347	25.606951
169.403983	5184.228630	25.611968
169.325025	5194.050305	25.616986
169.515896	5204.062803	25.622003
169.834035	5210.359691	25.627021
169.632357	5216.687504	25.632039
170.168413	5224.750310	25.637056
170.356173	5237.245807	25.642074
170.650904	5233.207184	25.647091
170.532614	5245.010662	25.652109
170.943950	5273.998995	25.657127
171.261336	5273.301488	25.662144
171.265594	5278.483951	25.667162
171.511819	5271.180144	25.672180
171.570224	5286.724572	25.677197
171.702729	5298.198314	25.682215
171.908232	5302.484275	25.687232
171.671808	5301.131029	25.692250
172.134906	5305.957948	25.697268
172.609606	5318.742306	25.702285
172.637592	5325.637010	25.707303
172.978889	5325.261604	25.712320
172.879359	5345.822394	25.717338
173.350121	5351.650659	25.722356
173.343208	5346.468748	25.727373
173.126864	5351.552290	25.732391
174.042996	5368.506355	25.737408
173.886334	5388.652148	25.742426
174.092145	5376.197050	25.747444
174.180670	5379.301321	25.752461
174.042811	5380.373282	25.757479
174.333254	5385.396565	25.762496
174.516781	5413.728214	25.767514
174.911650	5407.037687	25.772532
174.834027	5396.957617	25.777549
174.788778	5425.283054	25.782567
175.378281	5429.314882	25.787584
175.171312	5440.140818	25.792602
175.533309	5449.423398	25.797620
175.889905	5447.103250	25.802637
175.734810	5462.637515	25.807655
176.353330	5461.330956	25.812672
176.074926	5479.206693	25.817690
176.392593	5478.575289	25.822708
176.845186	5488.647029	25.827725
176.719769	5509.805378	25.832743
177.124231	5509.814098	25.837760
177.144732	5515.123904	25.842778
177.304493	5529.197099	25.847796
177.874037	5538.586353	25.852813
178.093652	5538.417747	25.857831
178.716757	5528.742192	25.862848
178.267000	5541.467122	25.867866
178.343690	5551.653901	25.872884
178.773528	5558.226212	25.877901
178.719309	5564.551806	25.882919
179.153576	5558.989624	25.887936
179.302505	5588.200762	25.892954
179.352466	5590.848351	25.897972
179.708573	5588.002934	25.902989
179.521182	5591.979905	25.908007
179.914835	5602.790008	25.913024
180.362203	5623.982853	25.918042
180.182944	5621.382791	25.923060
180.508369	5620.818620	25.928077
180.483732	5640.257663	25.933095
180.821059	5636.504089	25.938112
181.180354	5643.995433	25.943130
180.997379	5645.427727	25.948148
181.343337	5662.593067	25.953165
181.445340	5673.852391	25.958183
181.915302	5676.619489	25.963200
181.751510	5679.947527	25.968218
181.755383	5692.736100	25.973236
182.379917	5699.110054	25.978253
182.392001	5714.141964	25.983271
182.327683	5735.129039	25.988288
182.966151	5736.034701	25.993306
182.890292	5742.427744	25.998324
182.800770	5743.668152	26.003341
182.724539	5767.063387	26.008359
183.484400	5765.987806	26.013376
183.352199	5789.438809	26.018394
183.627614	5788.528486	26.023412
184.358324	5797.790402	26.028429
184.210159	5808.401288	26.033447
184.724181	5812.414208	26.038464
184.521640	5814.117543	26.043482
184.798890	5825.273140	26.048500
185.073526	5833.525248	26.053517
184.985411	5845.879445	26.058535
185.515218	5850.557658	26.063552
185.393210	5853.774063	26.068570
185.318516	5868.775591	26.073588
185.828155	5866.825431	26.078605
185.850208	5873.934800	26.083623
186.048737	5895.517332	26.088640
186.362322	5908.921131	26.093658
186.224728	5912.130676	26.098676
186.908728	5913.178459	26.103693
187.185499	5935.918493	26.108711
187.421245	5924.736313	26.113728
187.712981	5925.600935	26.118746
187.251446	5933.949760	26.123764
187.779645	5937.245209	26.128781
187.718883	5952.363440	26.133799
188.150212	5952.403946	26.138816
188.295591	5964.981860	26.143834
188.538669	5971.101663	26.148852
188.669106	5976.472974	26.153869
188.878384	5991.351209	26.158887
189.062041	6003.072186	26.163904
189.290794	6006.160456	26.168922
188.838206	6014.991442	26.173940
189.267425	6021.586105	26.178957
189.694207	6027.883452	26.183975
189.728401	6051.712135	26.188992
190.175194	6062.805966	26.194010
190.041527	6073.468188	26.199028
190.488278	6076.165952	26.204045
190.402484	6098.246350	26.209063
190.750589	6101.337723	26.214080
191.172360	6112.838208	26.219098
191.185517	6134.546268	26.224116
191.572252	6133.055920	26.229133
191.717221	6145.302454	26.234151
191.873334	6147.208732	26.239168
192.385867	6163.089199	26.244186
192.384274	6173.309029	26.249204
192.627790	6173.986316	26.254221
192.661029	6188.251172	26.259239
193.019260	6192.286044	26.264256
193.211251	6201.123846	26.269274
193.117473	6209.441864	26.274292
193.277079	6220.102105	26.279309
193.477693	6234.550381	26.284327
193.986557	6237.643523	26.289344
194.092817	6253.316452	26.294362
194.125176	6268.436110	26.299380
194.215199	6267.851815	26.304397
194.476581	6290.624837	26.309415
194.763729	6289.201370	26.314432
195.113197	6290.878748	26.319450
195.137150	6321.447760	26.324468
195.917867	6308.172133	26.329485
195.632798	6307.048964	26.334503
195.844718	6326.236239	26.339520
196.058818	6340.208221	26.344538
196.265126	6349.543886	26.349556
196.437511	6348.030718	26.354573
196.500609	6365.258614	26.359591
197.230076	6369.150162	26.364608
197.333277	6373.979495	26.369626
197.172815	6388.041092	26.374644
197.506636	6397.152466	26.379661
197.408885	6403.027193	26.384679
197.591823	6417.449419	26.389696
198.046079	6418.703829	26.394714
198.240255	6434.616006	26.399732
198.332895	6443.156908	26.404749
198.466002	6454.072164	26.409767
198.628740	6464.784823	26.414784
199.259051	6456.277170	26.419802
198.981795	6482.093301	26.424820
199.320272	6479.048222	26.429837
199.284737	6487.702521	26.434855
199.677723	6507.096335	26.439872
199.843374	6511.961056	26.444890
199.773760	6529.312706	26.449908
200.201361	6539.836643	26.454925
200.384496	6549.655153	26.459943
200.275366	6564.469278	26.464960
200.902896	6576.304661	26.469978
201.026310	6575.573051	26.474996
201.365858	6578.572993	26.480013
201.704253	6595.612214	26.485031
202.130834	6601.304910	26.490048
202.230916	6597.776273	26.495066
202.423364	6610.088558	26.500084
202.688659	6620.887529	26.505101
202.887159	6635.044302	26.510119
202.859727	6633.175084	26.515136
203.791372	6634.215796	26.520154
203.231637	6628.154591	26.525172
203.523357	6649.517148	26.530189
203.907468	6652.684586	26.535207
203.640853	6657.259376	26.540224
204.350852	6675.210708	26.545242
204.111974	6690.115743	26.550260
204.513245	6686.438770	26.555277
204.667373	6696.479566	26.560295
204.497251	6716.387463	26.565312
205.005318	6715.152658	26.570330
205.148097	6747.495529	26.575348
204.984352	6744.812370	26.580365
205.628279	6758.808087	26.585383
205.583406	6769.795557	26.590400
205.925764	6779.726480	26.595418
205.926308	6791.018360	26.600436
206.600668	6798.814912	26.605453
206.707272	6817.333375	26.610471
206.674358	6832.069756	26.615488
207.049476	6839.775661	26.620506
207.217960	6855.203374	26.625524
207.312102	6870.256665	26.630541
207.785752	6874.570345	26.635559
207.827610	6899.247349	26.640576
208.016695	6900.542545	26.645594
208.260828	6915.803412	26.650612
208.270754	6934.908288	26.655629
209.243362	6934.906460	26.660647
208.891351	6963.024708	26.665664
209.472061	6955.342604	26.670682
209.697526	6961.060060	26.675700
209.869012	6982.319304	26.680717
210.032847	6989.950771	26.685735
209.903424	6991.765003	26.690752
210.497873	7000.464164	26.695770
210.880645	7024.839962	26.700788
210.933447	7020.324228	26.705805
211.288566	7024.984455	26.710823
211.143759	7043.241546	26.715840
211.237669	7049.232867	26.720858
211.367192	7053.942262	26.725876
211.519086	7081.743365	26.730893
211.947627	7075.086742	26.735911
211.905878	7100.973589	26.740928
212.430496	7096.085927	26.745946
212.709784	7109.651596	26.750964
213.023296	7126.595474	26.755981
213.220298	7130.432003	26.760999
213.204215	7137.065405	26.766016
213.390408	7131.417720	26.771034
213.605391	7145.363486	26.776052
213.689436	7165.025860	26.781069
213.909603	7162.497265	26.786087
214.135527	7190.514730	26.791104
214.343659	7184.832675	26.796122
214.526883	7199.168921	26.801140
214.712877	7222.718238	26.806157
215.171014	7220.399936	26.811175
215.324840	7224.367301	26.816192
215.570986	7236.435667	26.821210
215.911522	7241.974276	26.826228
215.605023	7246.130487	26.831245
216.620703	7259.315236	26.836263
216.575377	7258.534336	26.841280
216.907309	7256.680386	26.846298
216.916750	7276.360762	26.851316
217.332188	7284.470593	26.856333
217.298591	7285.872789	26.861351
217.419715	7305.230666	26.866368
217.681162	7308.646186	26.871386
218.118455	7318.445156	26.876404
218.311344	7338.898682	26.881421
218.451041	7338.896105	26.886439
218.637146	7355.100411	26.891456
218.814219	7367.910499	26.896474
219.123349	7376.026948	26.901492
219.196535	7388.840860	26.906509
220.065857	7393.776840	26.911527
219.906752	7407.506706	26.916544
220.228374	7403.084211	26.921562
220.347114	7428.772520	26.926580
220.345871	7438.781217	26.931597
220.846851	7441.491514	26.936615
220.798035	7462.759513	26.941632
220.801732	7464.644708	26.946650
221.119301	7488.716148	26.951668
221.470059	7495.866355	26.956685
221.668496	7501.053635	26.961703
221.686413	7520.346150	26.966720
222.200047	7530.390191	26.971738
222.392521	7546.850428	26.976756
222.669694	7564.923260	26.981773
223.040320	7560.813990	26.986791
222.985875	7589.172382	26.991808
223.094921	7588.523451	26.996826
223.445055	7603.169567	27.001844
223.510107	7617.775454	27.006861
223.913698	7631.567545	27.011879
224.098764	7651.910914	27.016896
224.122760	7662.472480	27.021914
224.554201	7679.885804	27.026932
224.665409	7686.340035	27.031949
225.036615	7697.481402	27.036967
224.989170	7702.781919	27.041984
225.515346	7728.960175	27.047002
225.757326	7737.625142	27.052020
225.889449	7748.310654	27.057037
226.010815	7770.184996	27.062055
226.482413	7777.050657	27.067072
226.852318	7792.404190	27.072090
227.203680	7796.263379	27.077108
226.678276	7797.610757	27.082125
227.363772	7823.145230	27.087143
227.527156	7833.402623	27.092160
227.968875	7851.861304	27.097178
228.245026	7857.928316	27.102196
228.041876	7864.946670	27.107213
228.766691	7866.515615	27.112231
228.894366	7886.179535	27.117248
228.763961	7883.233079	27.122266
229.107806	7888.589407	27.127284
229.322658	7918.409916	27.132301
229.704722	7912.636583	27.137319
229.329288	7931.800930	27.142336
229.970270	7942.102218	27.147354
230.431838	7960.668808	27.152372
230.510984	7977.072628	27.157389
230.874327	7978.435960	27.162407
231.215845	7984.611145	27.167424
231.288265	8000.510387	27.172442
231.553165	7999.845094	27.177460
231.814743	8008.525082	27.182477
232.050215	8026.905464	27.187495
231.990750	8038.123087	27.192512
232.641969	8052.086450	27.197530
232.874974	8057.922001	27.202548
232.673014	8068.236870	27.207565
232.823637	8078.999101	27.212583
233.264965	8095.516389	27.217600
233.488754	8108.134226	27.222618
233.947210	8124.886602	27.227636
233.932415	8131.642303	27.232653
234.433312	8144.118982	27.237671
234.556762	8156.621127	27.242688
234.670257	8156.427533	27.247706
235.111367	8175.837479	27.252724
235.151841	8183.785340	27.257741
235.735408	8195.539418	27.262759
236.030518	8205.311272	27.267776
236.048552	8217.403965	27.272794
236.389148	8220.522999	27.277812
236.205449	8240.680816	27.282829
236.828083	8254.715259	27.287847
236.629578	8267.929331	27.292864
237.049135	8278.176114	27.297882
237.268049	8285.254763	27.302900
237.404714	8314.936924	27.307917
237.683197	8328.351735	27.312935
238.107289	8345.459788	27.317952
238.035054	8361.653528	27.322970
238.702063	8368.971560	27.327988
238.756405	8388.159051	27.333005
238.928916	8392.109437	27.338023
239.288486	8402.249645	27.343040
239.754529	8423.178469	27.348058
240.124668	8423.693894	27.353076
240.071252	8435.640243	27.358093
240.352492	8440.094128	27.363111
240.493181	8447.878224	27.368128
240.834561	8475.046193	27.373146
241.171269	8470.340473	27.378164
241.174189	8501.344109	27.383181
241.296560	8507.983521	27.388199
242.042116	8523.719079	27.393216
242.099908	8542.471349	27.398234
242.266505	8534.790876	27.403252
242.557056	8557.872692	27.408269
242.671662	8570.372687	27.413287
243.060515	8577.669114	27.418304
243.357358	8598.565519	27.423322
243.497887	8601.325447	27.428340
243.524181	8620.544643	27.433357
243.659787	8625.973503	27.438375
243.977970	8634.494792	27.443392
244.132436	8649.509057	27.448410
244.591231	8654.616593	27.453428
244.884786	8670.440509	27.458445
244.959778	8683.090521	27.463463
245.274418	8686.447120	27.468480
245.509475	8710.277256	27.473498
245.960184	8717.582414	27.478516
246.333066	8729.771157	27.483533
246.241632	8740.082341	27.488551
246.828879	8742.009738	27.493568
246.418182	8761.379427	27.498586
247.114213	8768.842516	27.503604
247.223656	8775.280150	27.508621
247.293434	8794.236335	27.513639
247.260405	8808.339625	27.518656
247.523134	8833.195754	27.523674
248.143175	8848.829522	27.528692
248.314055	8874.105041	27.533709
248.706489	8882.222652	27.538727
249.009840	8904.769535	27.543744
248.948000	8917.979638	27.548762
249.251059	8936.338850	27.553780
249.567366	8944.207556	27.558797
249.665515	8962.650347	27.563815
250.306702	8985.692072	27.568832
250.296496	9000.342403	27.573850
250.771204	9014.736019	27.578868
251.094968	9020.888553	27.583885
251.582752	9027.768623	27.588903
251.951156	9048.676617	27.593920
252.047022	9063.395316	27.598938
252.516827	9060.636826	27.603956
252.750225	9083.323947	27.608973
252.879854	9082.813350	27.613991
253.144018	9090.819955	27.619008
253.299271	9112.477826	27.624026
253.827554	9115.484830	27.629044
253.632065	9122.504828	27.634061
254.011350	9142.740747	27.639079
254.377797	9138.361565	27.644096
254.710088	9167.849857	27.649114
255.011969	9165.977036	27.654132
254.992348	9180.521953	27.659149
255.227654	9189.466114	27.664167
255.550089	9194.133972	27.669184
255.472290	9231.201739	27.674202
255.933678	9221.571227	27.679220
255.917409	9236.944385	27.684237
256.151172	9259.085762	27.689255
256.242182	9277.014886	27.694272
256.580851	9300.360807	27.699290
257.154443	9317.602714	27.704308
257.227137	9333.266112	27.709325
257.283934	9358.007464	27.714343
257.622061	9373.235434	27.719360
257.622537	9397.087303	27.724378
258.415710	9410.884200	27.729396
258.576006	9434.808932	27.734413
258.958639	9444.402411	27.739431
259.303237	9459.730229	27.744448
259.591390	9473.240513	27.749466
260.031827	9480.041172	27.754484
260.509379	9500.867092	27.759501
260.400768	9505.418895	27.764519
261.022645	9515.149282	27.769536
261.448837	9537.472683	27.774554
261.233939	9536.203732	27.779572
261.412417	9540.407874	27.784589
261.931826	9547.000117	27.789607
262.129659	9560.363927	27.794624
262.216747	9569.710190	27.799642
262.618869	9576.452634	27.804660
263.186507	9591.411997	27.809677
263.160135	9596.703349	27.814695
263.444743	9603.300606	27.819712
263.588322	9608.332218	27.824730
263.535812	9621.290835	27.829748
263.625617	9623.488181	27.834765
263.966185	9644.138436	27.839783
264.208860	9660.141132	27.844800
264.178275	9683.631452	27.849818
264.755127	9704.758685	27.854836
264.803566	9732.427903	27.859853
264.991881	9748.241157	27.864871
265.586604	9759.699909	27.869888
265.575180	9784.658041	27.874906
265.915569	9804.148878	27.879924
266.566782	9818.325717	27.884941
266.952879	9844.255687	27.889959
267.205150	9842.372095	27.894976
267.044086	9862.199681	27.899994
267.708777	9874.325241	27.905012
267.776780	9897.901970	27.910029
268.175654	9907.190519	27.915047
268.798332	9924.855892	27.920064
268.968751	9939.846667	27.925082
268.951518	9960.831502	27.930100
269.214920	9962.366756	27.935117
269.578260	9991.009245	27.940135
270.020499	9998.473960	27.945152
270.380070	10019.257057	27.950170
270.511388	10033.931386	27.955188
270.921021	10052.798927	27.960205
270.805402	10063.486814	27.965223
271.707756	10079.943240	27.970240
271.716265	10095.300512	27.975258
272.193461	10096.915413	27.980276
272.450513	10098.818857	27.985293
272.319350	10116.769150	27.990311
272.881175	10123.820217	27.995328
272.918383	10143.439645	28.000346
273.228720	10147.328262	28.005364
273.626982	10168.102784	28.010381
273.878235	10175.762276	28.015399
274.228612	10192.602468	28.020416
274.145089	10212.624060	28.025434
274.346898	10230.684809	28.030452
274.602409	10247.863772	28.035469
275.057674	10274.256474	28.040487
275.590998	10277.715873	28.045504
275.345894	10294.240338	28.050522
275.784197	10316.155509	28.055540
275.910953	10328.966847	28.060557
276.288163	10365.042506	28.065575
276.507232	10371.167985	28.070592
276.897518	10393.980679	28.075610
277.008996	10399.919927	28.080628
277.486095	10417.835264	28.085645
277.788219	10444.081056	28.090663
278.044747	10453.657411	28.095680
278.545166	10476.167581	28.100698
278.674128	10489.313513	28.105716
279.235348	10500.986335	28.110733
279.590995	10521.996055	28.115751
280.009265	10525.894475	28.120768
280.074672	10529.621252	28.125786
280.350489	10537.603806	28.130804
280.319272	10551.350641	28.135821
280.633639	10557.777920	28.140839
280.985159	10575.942694	28.145856
280.934083	10587.360820	28.150874
281.178361	10603.368918	28.155892
282.007954	10600.961091	28.160909
281.847665	10632.370867	28.165927
282.279942	10643.480551	28.170944
282.826922	10664.452485	28.175962
282.951207	10670.156510	28.180980
283.212163	10682.299877	28.185997
283.344759	10702.560477	28.191015
283.931276	10716.493559	28.196032
283.728068	10741.064201	28.201050
284.009524	10748.497580	28.206068
284.701804	10766.836221	28.211085
284.540448	10789.636787	28.216103
284.736047	10802.594677	28.221120
284.886400	10821.665973	28.226138
285.290564	10854.144054	28.231156
285.902755	10859.529454	28.236173
286.192810	10900.253360	28.241191
286.537368	10903.911958	28.246208
287.129243	10930.664451	28.251226
286.799839	10941.380425	28.256244
287.032509	10961.096916	28.261261
287.652724	10981.004552	28.266279
288.253726	10988.823205	28.271296
288.637733	11011.130426	28.276314
288.608026	11025.622738	28.281332
289.281225	11033.453099	28.286349
289.184607	11052.705787	28.291367
289.808508	11065.284151	28.296384
290.034692	11084.932534	28.301402
290.403964	11099.388812	28.306420
290.677809	11112.942238	28.311437
290.850683	11120.415822	28.316455
291.256107	11134.079850	28.321472
291.097672	11144.301238	28.326490
291.423307	11164.030952	28.331508
291.813285	11176.186427	28.336525
292.188617	11206.700300	28.341543
292.583208	11207.076267	28.346560
292.866572	11234.321541	28.351578
293.079905	11249.331644	28.356596
293.016956	11260.687604	28.361613
293.597036	11284.265904	28.366631
294.132568	11295.169858	28.371648
294.245487	11320.026266	28.376666
294.432336	11339.391528	28.381684
294.741410	11342.539248	28.386701
294.993573	11371.067865	28.391719
295.255138	11402.281672	28.396736
295.672906	11409.396549	28.401754
295.683819	11434.530020	28.406772
296.288511	11449.577957	28.411789
296.452604	11470.047036	28.416807
297.007277	11486.781494	28.421824
297.243229	11503.623876	28.426842
297.181375	11522.581424	28.431860
297.900479	11527.033824	28.436877
297.918654	11562.246600	28.441895
298.257974	11574.038874	28.446912
298.701293	11594.677777	28.451930
299.112233	11607.518730	28.456948
299.473058	11618.674008	28.461965
299.390220	11628.538087	28.466983
299.815989	11644.948947	28.472000
300.238052	11646.053126	28.477018
299.889014	11666.834300	28.482036
300.567723	11683.954990	28.487053
300.987581	11706.770950	28.492071
301.094379	11716.791216	28.497088
301.574678	11745.137758	28.502106
301.918112	11745.757004	28.507124
302.079215	11762.619924	28.512141
302.299213	11788.474149	28.517159
302.758111	11805.809417	28.522176
302.999267	11822.126524	28.527194
303.020497	11846.642782	28.532212
303.330824	11861.971473	28.537229
303.531964	11890.046159	28.542247
303.728593	11911.701732	28.547264
304.318054	11941.727712	28.552282
305.005889	11968.686660	28.557300
305.315705	11978.566329	28.562317
305.697740	12000.251214	28.567335
306.107709	12007.403892	28.572352
306.601562	12020.188903	28.577370
306.627958	12035.761733	28.582388
307.121145	12050.674257	28.587405
307.422643	12059.428629	28.592423
307.432990	12080.949797	28.597440
307.600404	12094.967627	28.602458
308.387008	12119.720059	28.607476
308.360460	12113.769408	28.612493
308.770838	12133.090742	28.617511
308.995042	12161.849150	28.622528
309.543660	12172.170046	28.627546
309.625255	12186.364471	28.632564
309.961466	12218.877028	28.637581
310.381418	12230.246714	28.642599
310.275504	12251.587218	28.647616
310.802497	12278.067453	28.652634
310.743528	12301.912174	28.657652
311.410734	12311.294803	28.662669
311.408069	12352.530963	28.667687
312.164677	12364.302023	28.672704
312.307963	12389.169226	28.677722
312.479981	12416.025191	28.682740
313.140689	12423.922914	28.687757
313.199901	12449.674008	28.692775
313.478257	12473.381201	28.697792
313.708639	12490.394150	28.702810
314.074059	12516.039511	28.707828
314.389181	12541.226775	28.712845
315.043906	12569.861068	28.717863
315.228799	12588.555242	28.722880
315.733426	12598.314796	28.727898
315.580276	12623.814501	28.732916
316.316275	12624.033144	28.737933
316.618456	12654.298678	28.742951
316.861619	12673.676700	28.747968
317.366584	12695.071114	28.752986
317.525084	12720.694313	28.758004
317.969577	12734.044353	28.763021
318.066622	12745.921707	28.768039
318.198879	12769.938754	28.773056
318.585878	12789.898255	28.778074
318.875657	12816.599862	28.783092
319.150112	12836.489798	28.788109
319.549885	12862.338040	28.793127
319.240143	12882.141917	28.798144
319.925834	12901.584071	28.803162
320.527009	12925.452818	28.808180
320.738721	12947.449250	28.813197
321.139109	12969.654025	28.818215
321.302387	12994.912826	28.823232
321.786017	13006.803607	28.828250
321.946746	13026.980506	28.833268
322.387245	13036.336469	28.838285
322.785611	13057.299864	28.843303
323.017211	13083.828729	28.848320
323.424582	13107.123085	28.853338
323.822159	13122.736380	28.858356
324.159239	13139.281629	28.863373
324.417685	13167.947895	28.868391
324.617075	13175.555147	28.873408
325.444786	13190.384988	28.878426
325.482610	13211.970868	28.883444
325.866837	13229.928338	28.888461
326.488289	13249.942581	28.893479
326.481065	13266.782916	28.898496
327.009311	13283.298248	28.903514
327.037122	13305.199524	28.908532
327.291035	13324.767233	28.913549
328.020749	13340.338373	28.918567
327.860824	13372.095362	28.923584
328.304221	13381.077542	28.928602
328.592719	13409.587966	28.933620
329.016447	13430.325432	28.938637
329.390196	13458.419958	28.943655
329.776241	13467.406950	28.948672
330.047136	13492.719630	28.953690
330.249263	13517.436978	28.958708
330.954649	13536.980649	28.963725
331.503385	13549.948480	28.968743
331.620268	13574.754096	28.973760
331.915086	13587.786047	28.978778
332.476160	13614.812840	28.983796
332.674600	13626.111426	28.988813
333.050199	13645.985611	28.993831
333.147700	13663.256602	28.998848
333.630253	13676.512863	29.003866
333.774597	13694.696516	29.008884
333.935164	13720.888303	29.013901
334.400827	13739.291472	29.018919
334.762632	13770.966036	29.023936
334.972561	13787.544021	29.028954
335.260300	13812.110533	29.033972
335.470306	13835.123394	29.038989
336.231393	13864.558737	29.044007
336.124315	13888.599706	29.049024
336.722902	13909.132327	29.054042
337.260637	13934.005945	29.059060
337.479357	13958.516332	29.064077
337.985737	13972.114040	29.069095
337.953352	14001.676229	29.074112
338.597368	14009.620049	29.079130
338.821392	14042.711150	29.084148
339.087094	14069.845898	29.089165
339.566928	14085.810567	29.094183
339.422970	14118.281879	29.099200
340.168570	14133.348396	29.104218
340.561289	14158.780635	29.109236
340.499964	14181.389719	29.114253
341.136797	14208.538922	29.119271
341.450951	14231.758902	29.124288
342.071758	14245.334747	29.129306
342.412360	14266.667021	29.134324
342.248147	14294.038779	29.139341
342.817059	14313.558691	29.144359
343.108348	14332.766809	29.149376
343.456497	14345.863038	29.154394
343.841073	14376.456981	29.159412
344.022026	14405.005854	29.164429
344.530588	14417.245004	29.169447
344.723934	14448.425508	29.174464
345.034345	14456.560303	29.179482
345.519196	14490.033103	29.184500
345.632379	14508.318957	29.189517
346.123977	14520.228441	29.194535
346.140960	14557.744221	29.199552
346.689571	14580.884914	29.204570
347.199026	14603.285057	29.209588
347.566760	14629.535422	29.214605
348.214328	14650.845762	29.219623
348.301680	14677.758860	29.224640
348.527523	14688.145817	29.229658
348.886956	14718.191352	29.234676
349.084921	14745.897944	29.239693
349.576269	14767.308367	29.244711
349.632747	14802.818099	29.249728
350.455399	14821.031011	29.254746
350.967911	14847.924458	29.259764
351.186384	14871.561512	29.264781
351.633955	14890.452838	29.269799
352.269028	14911.067368	29.274816
352.301110	14935.614834	29.279834
352.938260	14955.483573	29.284852
353.252002	14980.482543	29.289869
353.708296	14990.959217	29.294887
353.818894	15016.844545	29.299904
354.084439	15032.273473	29.304922
354.616481	15062.666189	29.309940
355.124332	15086.257235	29.314957
355.121336	15096.532593	29.319975
355.538999	15131.037578	29.324992
355.690123	15146.009557	29.330010
355.935130	15180.418706	29.335028
356.233167	15204.139215	29.340045
356.817876	15229.516124	29.345063
357.208597	15259.155554	29.350080
357.737242	15287.999897	29.355098
358.348202	15302.369481	29.360116
358.088338	15325.421219	29.365133
358.866949	15344.601882	29.370151
359.198586	15377.495031	29.375168
359.643651	15403.571492	29.380186
360.145290	15415.189955	29.385204
360.054403	15445.514675	29.390221
360.554970	15467.547072	29.395239
360.898980	15494.959655	29.400256
361.269594	15513.698938	29.405274
361.754436	15534.638590	29.410292
361.807963	15572.071824	29.415309
362.401309	15581.995024	29.420327
362.810268	15614.380930	29.425344
363.188532	15636.714355	29.430362
363.423656	15660.392344	29.435380
363.975802	15691.687627	29.440397
364.328356	15712.397209	29.445415
364.889784	15733.947035	29.450432
364.784664	15755.796347	29.455450
365.426490	15777.922420	29.460468
365.693995	15803.991074	29.465485
365.788236	15827.672130	29.470503
366.277178	15845.455945	29.475520
366.432766	15876.527189	29.480538
366.855427	15889.765213	29.485556
367.374136	15919.972577	29.490573
367.938669	15939.550320	29.495591
368.214649	15958.855871	29.500608
368.478694	15985.702459	29.505626
368.822179	16003.869896	29.510644
368.760428	16036.380245	29.515661
369.514746	16049.305008	29.520679
369.841721	16085.141571	29.525696
370.250606	16112.235504	29.530714
370.436760	16131.835117	29.535732
370.894777	16171.888663	29.540749
371.333162	16183.529173	29.545767
371.975335	16219.389522	29.550784
372.733911	16240.265854	29.555802
372.951162	16253.337985	29.560820
373.110361	16272.237645	29.565837
373.469695	16290.855158	29.570855
373.846568	16317.891677	29.575872
374.093886	16343.411262	29.580890
374.901934	16347.186699	29.585908
375.132211	16379.195430	29.590925
375.375267	16395.036032	29.595943
375.726630	16405.285083	29.600960
375.709065	16452.974591	29.605978
376.362599	16471.007689	29.610996
376.680191	16500.949913	29.616013
377.397034	16528.687120	29.621031
377.523159	16559.517050	29.626048
377.654956	16583.032193	29.631066
378.229469	16604.959299	29.636084
378.478523	16632.014334	29.641101
379.006517	16657.158510	29.646119
379.532317	16679.716409	29.651136
379.755286	16710.183810	29.656154
380.431052	16732.587706	29.661172
380.723085	16767.072772	29.666189
381.275504	16786.858447	29.671207
381.762361	16805.315146	29.676224
381.750700	16838.146647	29.681242
382.094547	16863.160830	29.686260
382.062142	16890.669554	29.691277
382.635498	16915.972128	29.696295
383.306885	16943.271461	29.701312
383.500755	16975.490714	29.706330
384.142107	16994.133281	29.711348
384.086866	17026.680750	29.716365
384.630504	17053.236894	29.721383
385.109085	17077.537100	29.726400
385.286423	17118.670305	29.731418
385.948983	17136.508750	29.736436
386.255478	17180.737129	29.741453
386.656650	17213.029726	29.746471
387.351368	17242.076997	29.751488
387.362161	17262.301249	29.756506
387.702695	17290.436197	29.761524
388.269697	17311.972977	29.766541
388.609131	17343.054380	29.771559
389.055437	17367.374540	29.776576
389.305705	17406.998860	29.781594
389.719177	17431.212626	29.786612
390.118088	17462.949632	29.791629
390.048868	17496.701517	29.796647
390.831846	17522.600871	29.801664
391.034056	17559.936750	29.806682
391.749278	17585.752835	29.811700
392.350531	17618.377249	29.816717
392.615392	17635.099773	29.821735
393.349708	17657.722233	29.826752
393.225618	17686.078195	29.831770
393.853552	17698.741428	29.836788
394.323949	17725.254021	29.841805
394.816108	17754.115020	29.846823
395.106165	17758.715842	29.851840
395.446690	17791.043246	29.856858
395.661466	17809.509837	29.861876
395.994489	17831.313016	29.866893
396.136611	17857.746156	29.871911
396.974818	17892.378054	29.876928
396.958044	17925.288214	29.881946
397.260591	17944.689423	29.886964
397.514774	17983.356015	29.891981
397.977455	18011.349011	29.896999
398.609591	18048.356304	29.902016
398.848431	18073.197368	29.907034
399.543856	18110.042989	29.912052
399.914431	18135.209156	29.917069
400.457489	18168.159566	29.922087
400.575092	18205.061613	29.927104
400.986181	18230.853366	29.932122
401.505723	18262.843081	29.937140
401.777699	18293.418779	29.942157
402.173412	18326.212597	29.947175
403.266392	18350.911144	29.952192
403.074191	18390.402940	29.957210
403.760592	18413.940818	29.962228
403.764464	18449.769750	29.967245
404.388771	18486.686304	29.972263
404.893864	18507.664207	29.977280
405.143554	18550.121079	29.982298
405.338451	18569.321703	29.987316
406.134119	18599.598473	29.992333
406.289749	18632.749495	29.997351
407.089963	18674.683625	30.002368
407.253731	18710.048395	30.007386
407.808834	18724.627271	30.012404
408.000322	18767.058068	30.017421
408.663011	18796.348256	30.022439
409.168031	18824.488531	30.027456
409.508936	18859.163755	30.032474
410.178465	18883.215871	30.037492
410.204545	18920.875596	30.042509
410.411488	18946.446850	30.047527
411.226968	18982.383813	30.052544
411.405380	19020.819415	30.057562
411.920854	19043.043289	30.062580
412.154175	19081.870376	30.067597
412.459135	19109.487732	30.072615
413.035034	19138.293130	30.077632
413.332642	19170.018623	30.082650
413.837677	19203.753020	30.087668
414.476894	19240.834309	30.092685
414.982026	19269.471921	30.097703
415.408409	19294.203363	30.102720
415.995618	19335.296277	30.107738
416.390254	19361.943831	30.112756
416.488423	19388.355136	30.117773
416.939184	19419.630092	30.122791
417.525839	19438.555626	30.127808
417.512734	19486.685046	30.132826
417.916732	19511.939198	30.137844
418.785277	19539.774577	30.142861
419.111763	19576.031802	30.147879
419.942266	19606.375582	30.152896
419.628493	19635.690100	30.157914
420.165550	19660.733270	30.162932
420.455116	19687.403459	30.167949
420.976267	19717.691429	30.172967
421.503173	19730.949960	30.177984
421.458738	19758.301433	30.183002
422.127592	19797.356075	30.188020
422.411194	19822.997963	30.193037
422.850873	19864.056679	30.198055
423.374583	19882.807098	30.203072
423.349387	19933.752426	30.208090
423.623896	19969.659640	30.213108
424.301124	20005.949616	30.218125
424.546727	20044.419012	30.223143
425.355461	20073.264742	30.228160
425.712593	20112.177781	30.233178
426.153525	20142.080912	30.238196
426.711050	20192.727209	30.243213
426.835992	20230.531172	30.248231
427.559945	20257.902925	30.253248
427.614215	20296.975298	30.258266
428.589889	20330.243076	30.263284
428.536677	20364.497881	30.268301
428.945234	20408.780980	30.273319
429.922274	20446.225264	30.278336
430.273480	20478.948681	30.283354
430.665097	20516.138410	30.288372
431.149662	20548.524564	30.293389
431.600295	20584.690895	30.298407
432.303304	20613.618118	30.303424
432.959984	20646.092650	30.308442
433.142840	20689.824170	30.313460
433.463894	20718.691803	30.318477
433.585471	20751.214096	30.323495
434.110910	20785.299894	30.328512
434.604240	20811.293290	30.333530
435.077395	20847.398121	30.338548
435.780168	20877.986078	30.343565
435.478120	20928.174544	30.348583
436.627229	20950.649270	30.353600
436.881540	21001.851142	30.358618
437.353907	21030.687963	30.363636
437.954844	21070.286572	30.368653
438.316094	21106.202353	30.373671
438.739276	21140.513916	30.378688
439.361228	21170.978607	30.383706
439.561594	21211.689192	30.388724
439.643054	21236.428544	30.393741
440.451471	21286.648741	30.398759
440.940562	21310.943911	30.403776
441.347429	21354.640082	30.408794
441.814081	21384.003502	30.413812
442.650610	21417.064682	30.418829
442.663668	21461.043886	30.423847
443.202601	21487.677239	30.428864
443.597724	21519.605464	30.433882
443.723435	21564.739388	30.438900
444.310885	21612.819643	30.443917
444.435367	21649.747036	30.448935
445.052176	21682.443025	30.453952
445.845040	21715.827368	30.458970
445.921648	21761.670021	30.463988
446.421169	21800.558663	30.469005
446.952502	21833.451994	30.474023
447.708928	21878.260057	30.479040
448.307038	21914.050060	30.484058
448.491295	21944.178616	30.489076
449.207502	21975.920543	30.494093
449.266433	22014.180920	30.499111
450.103797	22039.480681	30.504128
450.305975	22062.123059	30.509146
450.499860	22090.935242	30.514164
451.309888	22121.854602	30.519181
451.558979	22156.704764	30.524199
452.256410	22184.145536	30.529216
452.513108	22214.186899	30.534234
452.793073	22247.821156	30.539252
453.517795	22271.648248	30.544269
453.659895	22304.433457	30.549287
454.311994	22343.022155	30.554304
455.037908	22373.364589	30.559322
454.922655	22406.334495	30.564340
455.732609	22438.198961	30.569357
455.843154	22477.233943	30.574375
456.193417	22516.590441	30.579392
457.025292	22551.540502	30.584410
457.390139	22588.468007	30.589428
457.903121	22612.611296	30.594445
458.190046	22657.458116	30.599463
458.497992	22684.683474	30.604480
459.346461	22729.678819	30.609498
459.753547	22778.074484	30.614516
460.171964	22803.706475	30.619533
460.509941	22849.863607	30.624551
461.033074	22893.173944	30.629568
461.454380	22929.622942	30.634586
461.856992	22966.579710	30.639604
462.109811	23008.277780	30.644621
462.776681	23056.192876	30.649639
463.469933	23096.913151	30.654656
463.864212	23140.589202	30.659674
464.226188	23169.421128	30.664692
464.952648	23212.274448	30.669709
465.315830	23248.875669	30.674727
465.844087	23296.117390	30.679744
466.435451	23334.076592	30.684762
466.574469	23374.269522	30.689780
467.283900	23412.404899	30.694797
467.614815	23456.655202	30.699815
467.951758	23496.569668	30.704832
468.424350	23536.557973	30.709850
468.722760	23580.981132	30.714868
469.380203	23622.597979	30.719885
469.938906	23662.420944	30.724903
470.624541	23708.973877	30.729920
471.008980	23745.362913	30.734938
471.341076	23789.115569	30.739956
472.011343	23822.350885	30.744973
472.282773	23873.929165	30.749991
472.801006	23913.052936	30.755008
473.490945	23950.864737	30.760026
473.689693	23995.217154	30.765044
474.474076	24033.672682	30.770061
474.447965	24076.416163	30.775079
475.002230	24122.031584	30.780096
475.996274	24160.358085	30.785114
476.176109	24210.668874	30.790132
476.858554	24245.148818	30.795149
477.299172	24289.174962	30.800167
478.206354	24318.111005	30.805184
478.531771	24343.547808	30.810202
479.165570	24382.517910	30.815220
479.046919	24418.698306	30.820237
479.766317	24457.484097	30.825255
480.365827	24497.731204	30.830272
481.174067	24531.266781	30.835290
481.205580	24571.601743	30.840308
481.805658	24596.605527	30.845325
482.191057	24630.943007	30.850343
482.276166	24667.938650	30.855360
482.866185	24690.761629	30.860378
483.379890	24738.877114	30.865396
483.981116	24765.032190	30.870413
484.247650	24797.519307	30.875431
484.529651	24846.225399	30.880448
484.955063	24876.708761	30.885466
485.494679	24933.383875	30.890484
486.029302	24966.287449	30.895501
486.198655	25015.391154	30.900519
486.554206	25061.231206	30.905536
487.416521	25093.311192	30.910554
487.521999	25147.097117	30.915572
488.291389	25199.738788	30.920589
488.750707	25244.581217	30.925607
488.850283	25293.082199	30.930624
489.845840	25336.760563	30.935642
490.516653	25392.311519	30.940660
490.744275	25441.879927	30.945677
491.125199	25488.628484	30.950695
491.615236	25525.155228	30.955712
492.358723	25566.705790	30.960730
492.479340	25629.221601	30.965748
493.345398	25666.711552	30.970765
493.996965	25716.106509	30.975783
494.239683	25763.758717	30.980800
495.240295	25807.664550	30.985818
495.166982	25861.482289	30.990836
495.861647	25905.713419	30.995853
496.512146	25948.589318	31.000871
497.156292	25992.939433	31.005888
497.704016	26039.472626	31.010906
498.351271	26091.112085	31.015924
498.603462	26123.143548	31.020941
499.068770	26168.870603	31.025959
499.283842	26217.967015	31.030976
500.282615	26250.953963	31.035994
500.428845	26304.418164	31.041012
501.210819	26351.519074	31.046029
501.779764	26394.226623	31.051047
502.194800	26437.783039	31.056064
502.861947	26481.698454	31.061082
503.601290	26534.245084	31.066100
504.201755	26570.623288	31.071117
504.830392	26607.015833	31.076135
504.834666	26653.933967	31.081152
505.765284	26685.176013	31.086170
505.834334	26722.380605	31.091188
506.313465	26767.987091	31.096205
506.476243	26817.014995	31.101223
506.971460	26856.641372	31.106240
507.398503	26905.534320	31.111258
507.893299	26966.112989	31.116276
508.677963	27008.395207	31.121293
509.073001	27056.694525	31.126311
509.279675	27114.539125	31.131328
510.034607	27157.744588	31.136346
510.366444	27212.732900	31.141364
510.964917	27266.882324	31.146381
511.767645	27309.484051	31.151399
512.343414	27358.700667	31.156416
513.081960	27394.291201	31.161434
513.403010	27441.007628	31.166452
513.970539	27485.765417	31.171469
515.133091	27526.456406	31.176487
515.012850	27572.848729	31.181504
515.845495	27606.935165	31.186522
516.116656	27650.726640	31.191540
516.673407	27678.407711	31.196557
517.069992	27719.115483	31.201575
517.017925	27761.045869	31.206592
517.733659	27801.007008	31.211610
518.189543	27849.427804	31.216628
518.640379	27889.344648	31.221645
519.699515	27931.489065	31.226663
519.624269	27984.868904	31.231680
520.374335	28026.884876	31.236698
521.007340	28081.226716	31.241716
521.399197	28123.838490	31.246733
521.746733	28161.476439	31.251751
522.132613	28228.020974	31.256768
522.792272	28270.456297	31.261786
523.123778	28318.952609	31.266804
523.682069	28366.726955	31.271821
524.093657	28421.194825	31.276839
524.627823	28478.339894	31.281856
525.404590	28525.835611	31.286874
525.923815	28583.715402	31.291892
526.443813	28649.220361	31.296909
527.150326	28688.664527	31.301927
527.618755	28748.506084	31.306944
528.307336	28792.095703	31.311962
528.582431	28838.438595	31.316980
528.946117	28894.335534	31.321997
529.488751	28943.312884	31.327015
530.336044	29004.900350	31.332032
531.215572	29052.998850	31.337050
531.749048	29109.947345	31.342068
531.988433	29159.385608	31.347085
532.657055	29216.132260	31.352103
533.029624	29267.700423	31.357120
533.755334	29305.133140	31.362138
533.966063	29359.447875	31.367156
534.341646	29415.092116	31.372173
534.895422	29465.290038	31.377191
535.561855	29526.492817	31.382208
536.149615	29590.781748	31.387226
536.652084	29647.074581	31.392244
537.011514	29696.813148	31.397261
538.039999	29760.632254	31.402279
538.197798	29804.305911	31.407296
539.007479	29860.094277	31.412314
539.727860	29910.439432	31.417332
540.020714	29975.172944	31.422349
541.108438	30018.841555	31.427367
541.424303	30066.786859	31.432384
542.139296	30122.433975	31.437402
542.305478	30172.767464	31.442420
543.147762	30223.654948	31.447437
543.554548	30270.124968	31.452455
544.326182	30328.577691	31.457472
544.891639	30371.049475	31.462490
545.246118	30419.042987	31.467508
545.757481	30467.341958	31.472525
546.298486	30505.281067	31.477543
546.750065	30571.069558	31.482560
547.250269	30620.288937	31.487578
547.563318	30664.361830	31.492596
548.367089	30717.181753	31.497613
548.809936	30760.220605	31.502631
549.382249	30833.915865	31.507648
549.823692	30883.243511	31.512666
550.383034	30935.170597	31.517684
550.842898	30998.021828	31.522701
551.452826	31042.888985	31.527719
552.028154	31092.516896	31.532736
552.534302	31132.435136	31.537754
553.197532	31186.768989	31.542772
553.415521	31241.646808	31.547789
554.070157	31288.851541	31.552807
554.737333	31346.813776	31.557824
555.384050	31385.390431	31.562842
555.889360	31447.551048	31.567860
556.132335	31499.289182	31.572877
556.895936	31549.054456	31.577895
557.350313	31609.210986	31.582912
558.065394	31658.116885	31.587930
558.651966	31713.301200	31.592948
559.104599	31765.071684	31.597965
560.011010	31814.911894	31.602983
560.509339	31875.194581	31.608000
560.860149	31921.444714	31.613018
561.487118	31976.544283	31.618036
561.454727	32045.759884	31.623053
562.382230	32091.337608	31.628071
562.880854	32163.984080	31.633088
563.542370	32214.582213	31.638106
563.980541	32274.690042	31.643124
564.509601	32332.902394	31.648141
565.220811	32392.842385	31.653159
565.735498	32454.762015	31.658176
566.353659	32506.920643	31.663194
567.201247	32575.882271	31.668212
567.601999	32633.990620	31.673229
568.154377	32694.645807	31.678247
568.679247	32752.509967	31.683264
569.070984	32822.365252	31.688282
570.024750	32878.129854	31.693300
570.521692	32941.044952	31.698317
571.329646	32988.825248	31.703335
571.959218	33050.443944	31.708352
572.474091	33102.996923	31.713370
572.716855	33162.616258	31.718388
573.314178	33234.550233	31.723405
573.957456	33284.214061	31.728423
574.689039	33348.546512	31.733440
575.070512	33403.899395	31.738458
575.974889	33464.480032	31.743476
576.871400	33529.467467	31.748493
577.511140	33571.874685	31.753511
578.393807	33632.573090	31.758528
578.516288	33691.273702	31.763546
579.394148	33734.787422	31.768564
579.716613	33793.972817	31.773581
580.323494	33848.747005	31.778599
580.911795	33898.560492	31.783616
581.402779	33945.278673	31.788634
582.189437	34001.730834	31.793652
582.455857	34058.010476	31.798669
582.884772	34107.746776	31.803687
583.828970	34168.856540	31.808704
584.108322	34219.144908	31.813722
584.772333	34275.539331	31.818740
585.061712	34336.237301	31.823757
585.971939	34392.679720	31.828775
586.418692	34453.642384	31.833792
586.862274	34518.771471	31.838810
587.406580	34578.323544	31.843828
588.146371	34641.355931	31.848845
589.054943	34696.174318	31.853863
589.730862	34756.156495	31.858880
589.767633	34801.222642	31.863898
590.806977	34853.110157	31.868916
591.119044	34915.289598	31.873933
591.700559	34960.565828	31.878951
592.536917	35010.432889	31.883968
593.017332	35064.420649	31.888986
593.416931	35112.381491	31.894004
593.656886	35168.631122	31.899021
594.455633	35225.899374	31.904039
595.001242	35284.317431	31.909056
595.351860	35353.059562	31.914074
596.390139	35405.337036	31.919092
596.464845	35464.449003	31.924109
597.238757	35534.409439	31.929127
597.947482	35587.300577	31.934144
598.255525	35655.599596	31.939162
599.368065	35715.231850	31.944180
599.774230	35784.149486	31.949197
600.230416	35843.843415	31.954215
601.031102	35893.905036	31.959232
601.520998	35962.689570	31.964250
602.817986	36031.861591	31.969268
603.081034	36084.187237	31.974285
603.486443	36138.105410	31.979303
604.210256	36202.420979	31.984320
604.687245	36258.615857	31.989338
605.483767	36321.101888	31.994356
605.950455	36385.709985	31.999373
606.783152	36443.478319	32.004391
607.131900	36506.616651	32.009408
607.751398	36571.878708	32.014426
608.355077	36631.831739	32.019444
608.853002	36703.688742	32.024461
609.326665	36760.144537	32.029479
610.007510	36828.638806	32.034496
610.763993	36895.665794	32.039514
611.570793	36955.267511	32.044532
612.271980	37030.879685	32.049549
612.591352	37095.502061	32.054567
613.216423	37158.754762	32.059584
613.813511	37232.566978	32.064602
614.504111	37287.912226	32.069620
615.299619	37358.090777	32.074637
615.666984	37430.016444	32.079655
616.580549	37482.951837	32.084672
616.892371	37552.627237	32.089690
617.727990	37623.017963	32.094708
618.373912	37695.997014	32.099725
618.909815	37763.010038	32.104743
619.591949	37828.174716	32.109760
620.142920	37889.327429	32.114778
620.843465	37954.770434	32.119796
621.535482	38025.937706	32.124813
622.411302	38084.105000	32.129831
622.895066	38144.843569	32.134848
623.512577	38218.495427	32.139866
624.027427	38271.505392	32.144884
624.661440	38346.405002	32.149901
625.203160	38410.079874	32.154919
625.761980	38476.491994	32.159936
626.372582	38545.266341	32.164954
627.118422	38605.495919	32.169972
627.808944	38666.170452	32.174989
628.185524	38734.583345	32.180007
629.423548	38790.366586	32.185024
629.829418	38860.817407	32.190042
630.716678	38923.325785	32.195060
630.885025	38985.905964	32.200077
631.530568	39051.219953	32.205095
632.630912	39108.561059	32.210112
633.240810	39171.081447	32.215130
633.840107	39229.822142	32.220148
634.375188	39275.438810	32.225165
634.822221	39325.151722	32.230183
635.226638	39363.258433	32.235200
635.595500	39436.994214	32.240218
636.391459	39495.450690	32.245236
637.140232	39553.069163	32.250253
637.599554	39620.183740	32.255271
638.465694	39679.869782	32.260288
638.795039	39758.916688	32.265306
639.349942	39819.658516	32.270324
640.059651	39894.873925	32.275341
640.565567	39969.987615	32.280359
641.201327	40032.582422	32.285376
641.816194	40107.792295	32.290394
642.457095	40167.886530	32.295412
643.045151	40242.593143	32.300429
643.524006	40317.431770	32.305447
644.287467	40388.378581	32.310464
644.746314	40472.252880	32.315482
645.806112	40543.631107	32.320500
646.376367	40627.724446	32.325517
647.033893	40698.828881	32.330535
647.550325	40763.807273	32.335552
648.216643	40845.126573	32.340570
649.228377	40924.864289	32.345588
650.023644	40997.279312	32.350605
650.543698	41063.508311	32.355623
651.534480	41135.320122	32.360640
651.747362	41214.812409	32.365658
652.812932	41279.436582	32.370676
653.589970	41349.409330	32.375693
654.007628	41418.267384	32.380711
654.721271	41486.666315	32.385728
655.562078	41562.630836	32.390746
656.234806	41627.248602	32.395764
657.293924	41688.730847	32.400781
657.383240	41761.944420	32.405799
658.404704	41827.509143	32.410816
658.775791	41891.401087	32.415834
659.359522	41961.073471	32.420852
660.525244	42030.413054	32.425869
660.620369	42093.868307	32.430887
661.637639	42166.620562	32.435904
662.142887	42233.572864	32.440922
662.707343	42302.858231	32.445940
663.407778	42382.205403	32.450957
663.878629	42446.701559	32.455975
664.832699	42508.958471	32.460992
665.300698	42589.626804	32.466010
665.739419	42654.473132	32.471028
666.792059	42730.028519	32.476045
667.288006	42824.386208	32.481063
667.964113	42879.801209	32.486080
668.200336	42960.784172	32.491098
669.056435	43023.614695	32.496116
670.356281	43105.464239	32.501133
670.749559	43175.475776	32.506151
671.706455	43241.037223	32.511168
672.065047	43316.867671	32.516186
673.021373	43393.549908	32.521204
673.622617	43450.857616	32.526221
673.710051	43525.663421	32.531239
674.510536	43605.570731	32.536256
675.258199	43681.796116	32.541274
675.861391	43761.777776	32.546292
676.980563	43827.876459	32.551309
677.423168	43900.657928	32.556327
678.092939	43955.013110	32.561344
678.820115	44027.249119	32.566362
679.851095	44085.810658	32.571380
680.258840	44151.870300	32.576397
680.894277	44221.125782	32.581415
681.312857	44278.137860	32.586432
681.956064	44350.354271	32.591450
682.572477	44413.866934	32.596468
683.250773	44483.034196	32.601485
683.721044	44563.871698	32.606503
684.852064	44634.514984	32.611520
685.115437	44703.063346	32.616538
685.668781	44769.142120	32.621556
686.458766	44853.527625	32.626573
687.071045	44940.459524	32.631591
687.621238	45024.771789	32.636608
688.410616	45105.448311	32.641626
689.051323	45185.341412	32.646644
689.764440	45269.353103	32.651661
690.456271	45346.396527	32.656679
691.449254	45422.462086	32.661696
691.939309	45509.224205	32.666714
692.643320	45596.646029	32.671732
693.299043	45668.063360	32.676749
694.247960	45760.172558	32.681767
695.053971	45835.231810	32.686784
695.833847	45931.004389	32.691802
696.425490	46007.956562	32.696820
696.946203	46076.470497	32.701837
697.488268	46168.030053	32.706855
698.669439	46248.330862	32.711872
699.570250	46332.205704	32.716890
699.931785	46415.371187	32.721908
700.897533	46492.285546	32.726925
701.193662	46575.610970	32.731943
702.082143	46655.775609	32.736960
702.936902	46737.089329	32.741978
703.287927	46825.304691	32.746996
704.275728	46902.940232	32.752013
704.681778	46988.643002	32.757031
705.555998	47074.113972	32.762048
706.591000	47159.830317	32.767066
707.215530	47242.415896	32.772084
707.958549	47310.550129	32.777101
708.455679	47399.486114	32.782119
709.259151	47472.900617	32.787136
709.802721	47564.169792	32.792154
710.576563	47648.706214	32.797172
711.434353	47741.190642	32.802189
711.744159	47823.521307	32.807207
712.638748	47902.370102	32.812224
713.698729	47984.735274	32.817242
714.055824	48071.638460	32.822260
715.242647	48146.129068	32.827277
715.900041	48233.415979	32.832295
716.449632	48315.759629	32.837312
717.305454	48392.380871	32.842330
717.872780	48479.405882	32.847348
718.804854	48557.073168	32.852365
719.310247	48643.313298	32.857383
720.263410	48717.222611	32.862400
720.938903	48795.533372	32.867418
721.537939	48884.172000	32.872436
722.318699	48966.802349	32.877453
723.112789	49045.735644	32.882471
723.922256	49127.957676	32.887488
724.487981	49199.191524	32.892506
725.196977	49288.417066	32.897524
726.068180	49345.811644	32.902541
726.505317	49423.576940	32.907559
727.282850	49492.240677	32.912576
728.054794	49572.259959	32.917594
728.469880	49648.696975	32.922612
729.213084	49725.193721	32.927629
729.776225	49815.424938	32.932647
730.160418	49888.074749	32.937664
731.032513	49976.344761	32.942682
731.423193	50068.636570	32.947700
732.518570	50152.331744	32.952717
733.290244	50244.810892	32.957735
733.627396	50342.630747	32.962752
734.466706	50431.764219	32.967770
735.112018	50528.516995	32.972788
736.094699	50619.983887	32.977805
736.742925	50703.363752	32.982823
737.493693	50799.367650	32.987840
738.339011	50899.127749	32.992858
738.777026	50998.999955	32.997876
739.867483	51085.264774	33.002893
740.328098	51187.572672	33.007911
741.090609	51284.707824	33.012928
742.344716	51374.629858	33.017946
742.952764	51476.327375	33.022964
743.624568	51569.189451	33.027981
744.549679	51669.654176	33.032999
745.169496	51758.659480	33.038016
746.177097	51852.503428	33.043034
746.456166	51955.098090	33.048052
747.472655	52050.381920	33.053069
748.309934	52137.103927	33.058087
748.654815	52247.131366	33.063104
749.824310	52340.426522	33.068122
750.713345	52444.521229	33.073140
751.288913	52534.466091	33.078157
752.384466	52631.401242	33.083175
752.980566	52716.832670	33.088192
753.705895	52812.585354	33.093210
754.553951	52911.698253	33.098228
755.522105	52997.176767	33.103245
756.189073	53096.491138	33.108263
756.813577	53187.757667	33.113280
757.809539	53276.448629	33.118298
758.398491	53377.868574	33.123316
759.104694	53462.280478	33.128333
759.655010	53562.027170	33.133351
760.569013	53653.203751	33.138368
761.591410	53746.403576	33.143386
762.015432	53853.811239	33.148404
763.057810	53955.512981	33.153421
764.055140	54034.344460	33.158439
764.588093	54134.160106	33.163456
765.582863	54219.607948	33.168474
765.938613	54318.840967	33.173492
766.800207	54406.194499	33.178509
767.613241	54511.873364	33.183527
768.376859	54612.026056	33.188544
769.500619	54686.428996	33.193562
770.316764	54794.623589	33.198580
771.004520	54875.354624	33.203597
771.503609	54974.782055	33.208615
772.198184	55065.211646	33.213632
773.258966	55148.902357	33.218650
774.065256	55256.684081	33.223668
774.618569	55344.446591	33.228685
775.559782	55430.571985	33.233703
776.082437	55524.109290	33.238720
776.814875	55595.806476	33.243738
777.012838	55680.912207	33.248756
778.022675	55776.328926	33.253773
778.612647	55862.071975	33.258791
779.148302	55960.436739	33.263808
780.100727	56056.205514	33.268826
780.621895	56166.118234	33.273844
781.399654	56258.081308	33.278861
782.427818	56358.451818	33.283879
783.374996	56468.289423	33.288896
784.063601	56555.352448	33.293914
784.708242	56664.501849	33.298932
785.364028	56768.784314	33.303949
786.297685	56864.054550	33.308967
786.862941	56975.120829	33.313984
787.921101	57074.630577	33.319002
788.535791	57180.969402	33.324020
789.270425	57288.837166	33.329037
790.161831	57396.578472	33.334055
790.821604	57511.196162	33.339072
792.086500	57616.936850	33.344090
792.804821	57720.872686	33.349108
793.474107	57824.456965	33.354125
794.485823	57933.533610	33.359143
794.926123	58052.633260	33.364160
795.820433	58158.589764	33.369178
796.636540	58272.187456	33.374196
797.756843	58377.128202	33.379213
798.744371	58477.718283	33.384231
799.265831	58597.705118	33.389248
800.375323	58692.942317	33.394266
801.058586	58806.963135	33.399284
801.663113	58909.558872	33.404301
802.616457	59017.766280	33.409319
803.640987	59132.832136	33.414336
804.677315	59228.109241	33.419354
805.429059	59339.170367	33.424372
805.862224	59439.496698	33.429389
806.775928	59542.120345	33.434407
807.697532	59652.327182	33.439424
808.484884	59749.992636	33.444442
809.348806	59871.832709	33.449460
810.225183	59978.654933	33.454477
811.030784	60074.966437	33.459495
811.745562	60192.579667	33.464512
812.513625	60292.267048	33.469530
813.105826	60407.203076	33.474548
814.060537	60519.216723	33.479565
814.948901	60627.544593	33.484583
815.784385	60738.055975	33.489600
816.748845	60844.937703	33.494618
817.148505	60954.264589	33.499636
818.218856	61062.539390	33.504653
819.152621	61182.625000	33.509671
819.596067	61292.110783	33.514688
820.908870	61393.559036	33.519706
821.187943	61505.841536	33.524724
822.153754	61619.540653	33.529741
823.426498	61720.990836	33.534759
824.066808	61839.049350	33.539776
825.044751	61940.802205	33.544794
825.546131	62052.905557	33.549812
826.530093	62159.013478	33.554829
827.599897	62270.139099	33.559847
827.908814	62378.565756	33.564864
828.919146	62490.568357	33.569882
829.763469	62597.099849	33.574900
830.395899	62694.773401	33.579917
831.193319	62798.355502	33.584935
832.141103	62901.970143	33.589952
833.057847	63010.963303	33.594970
833.840292	63103.607737	33.599988
834.499684	63218.459919	33.605005
835.608702	63310.476052	33.610023
836.591053	63417.519929	33.615040
837.280150	63519.271470	33.620058
837.793848	63614.219300	33.625076
838.888325	63731.025156	33.630093
839.696039	63834.301010	33.635111
840.178805	63954.976775	33.640128
841.217464	64046.135478	33.645146
842.180705	64162.801119	33.650164
842.622232	64274.825292	33.655181
843.669124	64387.666556	33.660199
844.448450	64506.912087	33.665216
845.407780	64628.252558	33.670234
846.277013	64739.487844	33.675252
846.910538	64853.556845	33.680269
847.885471	64970.029114	33.685287
848.375928	65091.753268	33.690304
849.306441	65211.123224	33.695322
850.120302	65338.503814	33.700340
850.900031	65468.248844	33.705357
851.662599	65585.701613	33.710375
852.645549	65703.055376	33.715392
853.596759	65836.137544	33.720410
854.426808	65959.378411	33.725428
855.285569	66084.315858	33.730445
856.472110	66210.382052	33.735463
857.259148	66336.154719	33.740480
858.419689	66458.528320	33.745498
859.395615	66586.269018	33.750516
860.220411	66702.295279	33.755533
861.506485	66814.793987	33.760551
861.945555	66941.051407	33.765568
862.525422	67049.982319	33.770586
863.994364	67168.945619	33.775604
864.680526	67281.267854	33.780621
865.691281	67394.763540	33.785639
866.561786	67513.865691	33.790656
867.522789	67630.000979	33.795674
868.389372	67754.099840	33.800692
869.132512	67865.865706	33.805709
870.222927	67974.906629	33.810727
870.666397	68096.301885	33.815744
871.900467	68211.598564	33.820762
872.760365	68334.165541	33.825780
873.499843	68451.353589	33.830797
874.160813	68562.966008	33.835815
874.988640	68681.253507	33.840832
876.041369	68797.772034	33.845850
877.144127	68930.658973	33.850868
877.586340	69050.466541	33.855885
878.769075	69164.771554	33.860903
879.586465	69284.486777	33.865920
880.400459	69399.416768	33.870938
881.628046	69523.213342	33.875956
882.205167	69644.279175	33.880973
883.442192	69757.402305	33.885991
883.990394	69876.374983	33.891008
884.783297	69997.090973	33.896026
885.744652	70118.159174	33.901044
886.786004	70233.435438	33.906061
887.517926	70352.962112	33.911079
888.403111	70473.096432	33.916096
889.268250	70583.939503	33.921114
890.265989	70698.972549	33.926132
890.719158	70803.846112	33.931149
892.296331	70907.579473	33.936167
892.745589	71018.550472	33.941184
893.572571	71137.313302	33.946202
894.996299	71237.949848	33.951220
895.250726	71356.321662	33.956237
896.031883	71470.401857	33.961255
897.033978	71585.875247	33.966272
897.942308	71707.814851	33.971290
898.681149	71823.434224	33.976308
899.664852	71951.812865	33.981325
900.545736	72063.584200	33.986343
901.234961	72196.692546	33.991360
901.906139	72324.125923	33.996378
903.389167	72453.013073	34.001396
904.057316	72584.008797	34.006413
904.799946	72702.351498	34.011431
905.562498	72844.937557	34.016448
906.806001	72967.208253	34.021466
907.535238	73099.531341	34.026484
908.385044	73228.723855	34.031501
909.273458	73360.105213	34.036519
910.474509	73493.921047	34.041536
911.135072	73630.369401	34.046554
912.227570	73764.603269	34.051572
913.328025	73897.293528	34.056589
914.325469	74027.522504	34.061607
915.072120	74148.908049	34.066624
915.529668	74302.817695	34.071642
916.970269	74420.598933	34.076660
917.840165	74564.803837	34.081677
919.062700	74691.982778	34.086695
919.393918	74828.347591	34.091712
920.573607	74965.312912	34.096730
921.731598	75099.657966	34.101748
922.388273	75235.743796	34.106765
923.444972	75373.680693	34.111783
924.525565	75510.457078	34.116800
925.274720	75645.922972	34.121818
926.336133	75773.381469	34.126836
927.506859	75927.538719	34.131853
928.841708	76055.491237	34.136871
929.658582	76169.754502	34.141888
930.398269	76303.252616	34.146906
931.427462	76423.547701	34.151924
932.454422	76556.215536	34.156941
933.657971	76679.310459	34.161959
934.393780	76805.247474	34.166976
935.139512	76939.323996	34.171994
936.326803	77067.604036	34.177012
936.896679	77209.921329	34.182029
938.113701	77327.647517	34.187047
939.063579	77466.462681	34.192064
939.436839	77607.910511	34.197082
940.759101	77721.902093	34.202100
941.632232	77865.590296	34.207117
942.621980	77996.381571	34.212135
943.633371	78124.133809	34.217152
944.364278	78258.296609	34.222170
945.594415	78386.305144	34.227188
946.544889	78536.076348	34.232205
947.273876	78662.746077	34.237223
948.368229	78796.010684	34.242240
949.133901	78929.969327	34.247258
949.929875	79058.508937	34.252276
951.138246	79193.749650	34.257293
951.678964	79317.240709	34.262311
952.816224	79436.775042	34.267328
953.743567	79563.454992	34.272346
954.671228	79687.738085	34.277364
955.350338	79822.532384	34.282381
956.444567	79944.929522	34.287399
957.544748	80066.016855	34.292416
958.203158	80195.793953	34.297434
959.483083	80326.791171	34.302452
959.942452	80458.449900	34.307469
960.911000	80600.058472	34.312487
962.162299	80735.415177	34.317504
962.816215	80873.237480	34.322522
964.136406	80999.651733	34.327540
964.748134	81153.861416	34.332557
965.664746	81296.672258	34.337575
966.993225	81424.599496	34.342592
967.407226	81569.386743	34.347610
968.543932	81711.670326	34.352628
969.194563	81863.012478	34.357645
970.964881	82010.159453	34.362663
971.613638	82157.062624	34.367680
972.626025	82294.347079	34.372698
973.536392	82444.770723	34.377716
974.290548	82592.127424	34.382733
975.211704	82746.828114	34.387751
976.474876	82892.280467	34.392768
977.300308	83047.138194	34.397786
978.438507	83195.131203	34.402804
979.509509	83346.318711	34.407821
980.437498	83503.225115	34.412839
981.891772	83636.572413	34.417856
982.598642	83796.060818	34.422874
984.155035	83934.454578	34.427892
984.451350	84086.989824	34.432909
985.663983	84245.942145	34.437927
986.597951	84383.745521	34.442944
987.594039	84531.846507	34.447962
988.566778	84685.824010	34.452980
989.999401	84828.115863	34.457997
990.870526	84976.892059	34.463015
992.114533	85124.715386	34.468032
993.022541	85273.923970	34.473050
994.222284	85408.645972	34.478068
995.304025	85552.715013	34.483085
996.330258	85703.349464	34.488103
997.806852	85836.148871	34.493120
998.459103	85976.178605	34.498138
999.369290	86111.079084	34.503156
1000.123949	86261.888584	34.508173
1001.064170	86403.588060	34.513191
1002.166922	86542.122938	34.518208
1003.048247	86705.228199	34.523226
1004.141218	86832.059933	34.528244
1005.185641	86985.540812	34.533261
1006.190212	87131.726839	34.538279
1007.380489	87271.643683	34.543296
1007.987874	87423.256983	34.548314
1009.227878	87569.659913	34.553332
1010.166344	87712.342066	34.558349
1011.212448	87857.646110	34.563367
1012.437195	88010.603907	34.568384
1013.320139	88159.480555	34.573402
1014.170143	88292.504993	34.578420
1015.213089	88440.230518	34.583437
1015.920585	88594.771077	34.588455
1017.295825	88729.350150	34.593472
1018.179632	88894.128105	34.598490
1019.328305	89029.689269	34.603508
1019.974436	89161.897933	34.608525
1020.965402	89291.069583	34.613543
1022.006000	89431.998493	34.618560
1022.906412	89582.248106	34.623578
1023.476748	89720.636435	34.628596
1024.833547	89864.249573	34.633613
1025.624176	90015.146589	34.638631
1026.821063	90160.522007	34.643648
1027.473014	90312.760199	34.648666
1028.671065	90467.383630	34.653684
1029.873169	90616.121543	34.658701
1030.800297	90771.848644	34.663719
1031.573181	90922.488468	34.668736
1032.191270	91086.679859	34.673754
1033.880124	91249.423189	34.678772
1035.132881	91415.410583	34.683789
1036.156399	91564.962344	34.688807
1037.262956	91719.621579	34.693824
1037.926932	91888.848823	34.698842
1038.833091	92047.144589	34.703860
1039.985888	92207.742438	34.708877
1040.837914	92376.441970	34.713895
1042.190888	92539.002643	34.718912
1043.164860	92724.950929	34.723930
1044.507671	92877.350508	34.728948
1045.835590	93050.083827	34.733965
1046.481585	93211.721505	34.738983
1048.001238	93361.759268	34.744000
1048.739508	93526.959978	34.749018
1049.658975	93689.903801	34.754036
1051.122130	93860.772216	34.759053
1051.870524	94030.633301	34.764071
1053.277111	94188.246201	34.769088
1053.943432	94350.666575	34.774106
1054.960376	94521.366487	34.779124
1056.320518	94688.181239	34.784141
1057.256838	94859.358902	34.789159
1058.391973	95019.414716	34.794176
1059.522596	95185.840334	34.799194
1060.523698	95358.618568	34.804212
1061.789245	95521.935051	34.809229
1062.854794	95694.249197	34.814247
1064.056283	95842.329000	34.819264
1065.233044	96016.095597	34.824282
1066.148338	96179.904768	34.829300
1067.542838	96337.818208	34.834317
1068.222610	96514.221570	34.839335
1069.630178	96669.134345	34.844352
1070.574500	96836.981833	34.849370
1071.676647	96993.979194	34.854388
1073.344422	97156.024422	34.859405
1073.948959	97320.170981	34.864423
1075.258602	97480.713862	34.869440
1075.907526	97648.470013	34.874458
1077.080146	97802.175159	34.879476
1078.330990	97965.111198	34.884493
1079.009184	98134.518068	34.889511
1080.459729	98300.772245	34.894528
1081.252710	98465.097691	34.899546
1082.151681	98630.520920	34.904564
1083.767773	98789.362768	34.909581
1084.501280	98949.142902	34.914599
1085.882132	99108.734713	34.919616
1086.997973	99285.598191	34.924634
1087.697529	99451.908107	34.929652
1088.836743	99614.803570	34.934669
1089.924161	99776.588016	34.939687
1090.761902	99931.994893	34.944704
1091.642648	100096.955831	34.949722
1093.168441	100256.670161	34.954740
1094.687139	100403.325080	34.959757
1095.197929	100561.600956	34.964775
1096.300361	100707.288087	34.969792
1097.252307	100875.002767	34.974810
1098.205493	101039.964129	34.979828
1099.583387	101178.548762	34.984845
1100.302835	101361.038552	34.989863
1101.430992	101523.017231	34.994880
1102.512675	101697.243725	34.999898
1103.422720	101869.682569	35.004916
1104.643188	102042.463811	35.009933
1105.342073	102215.300778	35.014951
1106.799859	102391.432625	35.019968
1107.942915	102567.427745	35.024986
1108.655010	102752.777908	35.030004
1110.170967	102926.130381	35.035021
1111.176985	103114.378893	35.040039
1112.323188	103282.849567	35.045056
1113.423481	103472.098203	35.050074
1114.938477	103653.478446	35.055092
1115.873776	103827.661103	35.060109
1116.979701	104012.910779	35.065127
1117.940769	104188.598645	35.070144
1119.136919	104381.953987	35.075162
1120.440082	104562.944946	35.080180
1121.474447	104741.258652	35.085197
1122.744060	104933.225435	35.090215
1124.007688	105116.620401	35.095232
1125.669371	105296.708574	35.100250
1126.770010	105476.675418	35.105268
1127.925429	105648.781974	35.110285
1128.601829	105832.506956	35.115303
1129.805403	106005.114476	35.120320
1131.165898	106177.798500	35.125338
1132.379061	106373.711362	35.130356
1133.314722	106545.910720	35.135373
1134.624651	106735.781385	35.140391
1135.873936	106913.770190	35.145408
1136.890372	107093.166594	35.150426
1137.712324	107275.395543	35.155444
1139.069852	107461.755006	35.160461
1139.943491	107644.915212	35.165479
1141.120591	107826.949867	35.170496
1142.482478	108014.135750	35.175514
1143.291968	108196.031010	35.180532
1144.895891	108385.370758	35.185549
1145.638433	108583.796877	35.190567
1146.905533	108767.444332	35.195584
1147.975064	108954.571067	35.200602
1149.137884	109144.293052	35.205620
1150.404211	109335.417956	35.210637
1151.551032	109525.727933	35.215655
1152.711395	109713.756913	35.220672
1154.145217	109900.804608	35.225690
1155.224659	110090.736987	35.230708
1156.402886	110275.182027	35.235725
1157.404680	110455.147846	35.240743
1158.530480	110649.776089	35.245760
1159.985679	110840.563621	35.250778
1161.042858	111027.123903	35.255796
1162.320757	111207.935761	35.260813
1163.327875	111400.688766	35.265831
1164.364965	111588.903009	35.270848
1165.638438	111775.660630	35.275866
1166.588063	111958.178529	35.280884
1167.945623	112140.313490	35.285901
1169.293763	112313.456669	35.290919
1169.615628	112485.769775	35.295936
1171.100474	112666.645645	35.300954
1172.236387	112844.185189	35.305972
1173.434476	113023.552547	35.310989
1174.339808	113215.612884	35.316007
1175.410333	113411.574580	35.321024
1176.451381	113593.441988	35.326042
1177.469533	113788.654848	35.331060
1178.944565	113978.738565	35.336077
1179.975032	114171.456238	35.341095
1181.055100	114365.066554	35.346112
1182.661979	114562.581971	35.351130
1183.432349	114760.743831	35.356148
1184.385918	114954.163724	35.361165
1186.005585	115161.424110	35.366183
1186.979252	115360.468784	35.371200
1188.338698	115559.058321	35.376218
1189.205952	115785.110305	35.381236
1190.646835	115984.956351	35.386253
1191.787952	116191.213746	35.391271
1192.655529	116398.341414	35.396288
1194.051317	116603.292671	35.401306
1195.292595	116827.897364	35.406324
1196.319899	117035.624093	35.411341
1197.394323	117259.170086	35.416359
1199.126596	117476.780564	35.421376
1200.466046	117678.454446	35.426394
1201.529610	117903.325000	35.431412
1202.785123	118106.219482	35.436429
1204.235247	118324.465865	35.441447
1205.140710	118536.620411	35.446464
1206.627341	118746.323593	35.451482
1207.631730	118968.335833	35.456500
1209.223754	119179.798709	35.461517
1210.382451	119392.487859	35.466535
1211.598737	119604.902936	35.471552
1212.538967	119810.066293	35.476570
1213.940016	120036.481532	35.481588
1215.089142	120252.245091	35.486605
1216.858695	120464.917096	35.491623
1217.536879	120675.515412	35.496640
1219.147897	120884.060217	35.501658
1219.949928	121106.514953	35.506676
1221.065784	121321.442806	35.511693
1222.812413	121527.194495	35.516711
1224.049273	121753.890850	35.521728
1225.282578	121971.452564	35.526746
1226.168647	122183.484601	35.531764
1227.455253	122400.064840	35.536781
1229.028119	122625.939260	35.541799
1230.157168	122845.640965	35.546816
1231.346361	123045.146125	35.551834
1232.500203	123271.322796	35.556852
1233.742288	123483.482630	35.561869
1235.017792	123716.904326	35.566887
1236.432496	123938.619898	35.571904
1237.475765	124154.733422	35.576922
1238.673507	124370.049866	35.581940
1239.995002	124591.202648	35.586957
1241.395015	124800.633460	35.591975
1242.331213	125034.615692	35.596992
1243.939431	125247.728628	35.602010
1244.963865	125466.199296	35.607028
1246.413997	125682.573296	35.612045
1247.466923	125888.583562	35.617063
1248.724936	126111.582971	35.622080
1250.021115	126319.343010	35.627098
1251.241572	126523.213217	35.632116
1252.264823	126727.168070	35.637133
1253.884010	126933.142446	35.642151
1254.747981	127140.535853	35.647168
1256.214880	127346.994454	35.652186
1257.360646	127551.010547	35.657204
1258.432781	127761.694544	35.662221
1259.761309	127981.298904	35.667239
1260.622962	128199.169426	35.672256
1262.126316	128398.759033	35.677274
1263.220450	128619.623462	35.682292
1264.602615	128848.478093	35.687309
1266.106505	129064.347176	35.692327
1266.980155	129280.968372	35.697344
1268.516091	129508.408082	35.702362
1269.650398	129727.042738	35.707380
1270.821473	129951.516430	35.712397
1272.060697	130178.870584	35.717415
1273.119779	130412.632224	35.722432
1274.753441	130637.908979	35.727450
1276.081785	130873.923904	35.732468
1277.151874	131109.450857	35.737485
1278.394898	131343.100202	35.742503
1279.667800	131575.440632	35.747520
1281.178280	131812.167635	35.752538
1282.623715	132042.226490	35.757556
1284.148418	132280.425101	35.762573
1285.714628	132510.873009	35.767591
1286.464672	132741.546199	35.772608
1288.139023	132967.821434	35.777626
1289.557220	133206.513541	35.782644
1290.929339	133429.837460	35.787661
1292.248756	133655.339459	35.792679
1293.348897	133897.220524	35.797696
1294.824559	134118.338853	35.802714
1295.987483	134349.487680	35.807732
1296.775099	134586.392474	35.812749
1298.288106	134824.218672	35.817767
1299.469163	135071.445089	35.822784
1300.876859	135307.935653	35.827802
1302.315039	135537.551340	35.832820
1303.600628	135786.984514	35.837837
1305.204587	136021.939046	35.842855
1306.185440	136266.494339	35.847872
1307.854615	136501.149882	35.852890
1309.377717	136744.985149	35.857908
1310.655028	136972.063597	35.862925
1311.906826	137202.659817	35.867943
1313.170652	137448.597024	35.872960
1314.213379	137682.375448	35.877978
1315.882467	137916.939507	35.882996
1317.145279	138162.818710	35.888013
1318.502184	138385.278363	35.893031
1319.823271	138630.809002	35.898048
1321.036083	138865.188790	35.903066
1322.666916	139106.360694	35.908084
1323.626737	139347.290179	35.913101
1325.385537	139574.864460	35.918119
1326.465195	139816.829863	35.923136
1327.970380	140045.273373	35.928154
1329.435901	140284.414108	35.933172
1330.623860	140530.132571	35.938189
1332.088235	140753.731102	35.943207
1333.296993	140993.324957	35.948224
1334.954812	141230.259487	35.953242
1335.911408	141466.880397	35.958260
1337.250467	141692.775484	35.963277
1338.735406	141915.414404	35.968295
1339.514643	142138.348904	35.973312
1340.871817	142359.591549	35.978330
1342.296812	142578.554535	35.983348
1343.411307	142807.435875	35.988365
1345.230898	143025.474142	35.993383
1346.191690	143261.028624	35.998400
1347.467954	143484.358726	36.003418
1348.541640	143713.607767	36.008436
1349.940841	143967.063678	36.013453
1351.436653	144194.077573	36.018471
1352.241627	144434.066022	36.023488
1353.473532	144678.512818	36.028506
1354.775197	144926.830319	36.033524
1356.128211	145188.228530	36.038541
1357.554489	145450.402806	36.043559
1358.527715	145695.863105	36.048576
1359.932687	145958.526513	36.053594
1360.765975	146229.440852	36.058612
1362.101199	146488.302343	36.063629
1364.019794	146761.488946	36.068647
1365.118950	147031.553670	36.073664
1366.522941	147301.430510	36.078682
1368.101178	147567.754812	36.083700
1369.565700	147844.309325	36.088717
1370.970674	148112.479825	36.093735
1372.100880	148383.893745	36.098752
1373.771803	148661.523686	36.103770
1375.223451	148926.965571	36.108788
1376.322419	149213.889319	36.113805
1378.140543	149489.865017	36.118823
1379.537371	149763.312316	36.123840
1380.598105	150049.373663	36.128858
1382.243585	150315.820751	36.133876
1383.636663	150610.646437	36.138893
1385.031898	150880.398545	36.143911
1386.527598	151160.422467	36.148928
1387.928046	151430.076162	36.153946
1389.837818	151711.113847	36.158964
1390.686869	151987.331404	36.163981
1392.690967	152255.178847	36.168999
1393.954747	152547.491435	36.174016
1395.249609	152816.081529	36.179034
1396.790533	153094.513947	36.184052
1397.837493	153374.958039	36.189069
1399.179501	153653.490779	36.194087
1400.733287	153939.474454	36.199104
1402.235854	154219.874732	36.204122
1403.626555	154484.109692	36.209140
1405.326773	154782.303508	36.214157
1406.591950	155045.256452	36.219175
1408.387764	155330.601427	36.224192
1409.531389	155603.371070	36.229210
1411.216131	155882.345064	36.234228
1412.283424	156154.902786	36.239245
1413.792695	156428.302690	36.244263
1414.933478	156712.763711	36.249280
1416.418084	156993.947794	36.254298
1417.898934	157274.474813	36.259316
1419.353629	157563.837424	36.264333
1420.839586	157831.707066	36.269351
1422.219961	158121.149383	36.274368
1423.604504	158404.376911	36.279386
1425.218151	158685.297734	36.284404
1426.441449	158964.851453	36.289421
1427.794594	159249.396722	36.294439
1429.382627	159525.253024	36.299456
1430.726193	159802.280672	36.304474
1432.346717	160072.058443	36.309492
1433.223510	160341.072806	36.314509
1434.847680	160613.048292	36.319527
1435.978127	160876.442045	36.324544
1437.520892	161139.921572	36.329562
1438.942028	161419.598758	36.334580
1440.298152	161695.951855	36.339597
1441.866849	161966.613174	36.344615
1443.180582	162249.295109	36.349632
1444.640361	162538.704452	36.354650
1446.234365	162810.458103	36.359668
1446.981387	163087.162002	36.364685
1448.774794	163373.210464	36.369703
1450.199535	163664.244566	36.374720
1451.400122	163960.164399	36.379738
1453.099887	164249.203105	36.384756
1454.311976	164553.067685	36.389773
1455.831410	164838.803209	36.394791
1457.602871	165139.851549	36.399808
1458.784461	165435.657717	36.404826
1460.065410	165731.094196	36.409844
1461.683682	166028.710074	36.414861
1463.345166	166332.220944	36.419879
1464.755992	166635.711876	36.424896
1466.029808	166946.142815	36.429914
1467.854298	167238.898404	36.434932
1469.262453	167552.940340	36.439949
1470.797763	167868.029334	36.444967
1472.048455	168167.369820	36.449984
1473.517441	168480.481897	36.455002
1475.269853	168780.276485	36.460020
1476.801017	169099.854023	36.465037
1478.020395	169400.793984	36.470055
1479.882334	169723.950378	36.475072
1480.948120	170035.515528	36.480090
1483.113740	170347.218297	36.485108
1484.189156	170661.082893	36.490125
1485.693817	170972.378811	36.495143
1487.242059	171292.235236	36.500160
1488.628003	171611.790732	36.505178
1490.215478	171917.140394	36.510196
1492.061950	172237.867677	36.515213
1493.808534	172548.804156	36.520231
1495.271690	172854.802244	36.525248
1496.424704	173174.444878	36.530266
1498.407445	173477.391581	36.535284
1500.269558	173787.289136	36.540301
1501.462458	174105.167414	36.545319
1503.053085	174405.595882	36.550336
1504.358497	174720.616912	36.555354
1506.082970	175020.227557	36.560372
1507.303679	175334.606632	36.565389
1509.165462	175641.013403	36.570407
1510.754798	175950.284513	36.575424
1512.228647	176252.012734	36.580442
1513.592423	176562.708278	36.585460
1515.719860	176865.791732	36.590477
1517.065367	177177.890174	36.595495
1518.566092	177479.062971	36.600512
1519.862021	177779.789133	36.605530
1521.814558	178074.468937	36.610548
1523.208315	178383.267067	36.615565
1524.725058	178686.779680	36.620583
1526.434090	178983.078763	36.625600
1527.749954	179300.056145	36.630618
1528.971034	179597.365904	36.635636
1530.774369	179896.294598	36.640653
1532.297007	180191.882602	36.645671
1533.898422	180476.683610	36.650688
1535.219935	180780.520023	36.655706
1537.093010	181052.777421	36.660724
1538.301775	181342.394937	36.665741
1539.569081	181625.569295	36.670759
1541.425315	181905.703199	36.675776
1542.584767	182199.242843	36.680794
1544.393287	182491.052202	36.685812
1545.440491	182790.299947	36.690829
1546.806640	183092.035220	36.695847
1548.638467	183401.602901	36.700864
1550.181935	183707.843668	36.705882
1551.460904	183994.633386	36.710900
1553.302129	184313.508679	36.715917
1554.404671	184620.957093	36.720935
1556.205169	184928.786943	36.725952
1557.474749	185235.538437	36.730970
1559.167527	185556.907934	36.735988
1560.578856	185873.806914	36.741005
1562.290025	186190.988177	36.746023
1564.079679	186513.844987	36.751040
1565.125354	186840.710815	36.756058
1566.524027	187164.778355	36.761076
1568.331176	187501.309034	36.766093
1569.923757	187826.478033	36.771111
1571.482560	188147.059237	36.776128
1572.902377	188488.749948	36.781146
1574.696624	188813.078751	36.786164
1576.000340	189152.977278	36.791181
1577.726448	189492.554103	36.796199
1579.236075	189828.715793	36.801216
1580.918941	190175.133218	36.806234
1582.824758	190516.057206	36.811252
1584.288751	190856.167510	36.816269
1585.891739	191207.796165	36.821287
1587.618942	191541.608406	36.826304
1588.795698	191891.318373	36.831322
1590.595732	192237.487073	36.836340
1592.082499	192570.443318	36.841357
1593.675915	192925.561829	36.846375
1595.570650	193266.426849	36.851392
1596.724723	193619.057499	36.856410
1598.901044	193957.861244	36.861428
1600.504577	194311.754511	36.866445
1602.085677	194661.933733	36.871463
1604.092146	195003.919560	36.876480
1605.452370	195343.982702	36.881498
1607.166295	195686.921867	36.886516
1608.971839	196038.023662	36.891533
1610.398435	196384.162474	36.896551
1612.100096	196720.786668	36.901568
1613.650470	197077.966648	36.906586
1615.122792	197417.590393	36.911604
1616.898030	197765.583213	36.916621
1618.711779	198113.990444	36.921639
1620.542947	198462.142676	36.926656
1622.342987	198807.115113	36.931674
1623.825624	199150.630885	36.936692
1625.078491	199489.057055	36.941709
1626.394527	199836.476120	36.946727
1628.355872	200180.578140	36.951744
1629.889296	200533.982846	36.956762
1631.565046	200878.694116	36.961780
1633.458098	201220.108157	36.966797
1634.533327	201577.021834	36.971815
1637.000317	201923.600825	36.976832
1638.313761	202267.972364	36.981850
1640.152681	202608.932175	36.986868
1641.309225	202936.839673	36.991885
1643.033067	203259.334920	36.996903
1644.560599	203578.359647	37.001920
1645.937816	203926.042342	37.006938
1647.577716	204244.721240	37.011956
1649.566323	204575.114121	37.016973
1650.996333	204908.190948	37.021991
1652.524103	205251.893370	37.027008
1653.969965	205591.890559	37.032026
1655.793058	205929.769962	37.037044
1657.800907	206267.480647	37.042061
1659.066949	206613.759145	37.047079
1660.347331	206954.576868	37.052096
1661.933527	207316.131469	37.057114
1663.560383	207675.116074	37.062132
1665.560430	208022.587324	37.067149
1666.822287	208380.898906	37.072167
1668.615809	208746.082633	37.077184
1670.528129	209117.216358	37.082202
1671.798108	209479.137591	37.087220
1673.436013	209844.415375	37.092237
1674.840935	210217.885369	37.097255
1676.713781	210589.730553	37.102272
1678.215511	210973.498725	37.107290
1679.527466	211345.058906	37.112308
1681.624511	211736.173279	37.117325
1683.269575	212127.567242	37.122343
1685.180666	212510.385706	37.127360
1686.820589	212898.888713	37.132378
1688.685096	213284.867410	37.137396
1690.354652	213675.400638	37.142413
1691.980839	214070.996741	37.147431
1693.796691	214441.877080	37.152448
1695.483350	214844.628544	37.157466
1697.271760	215232.456618	37.162484
1699.277117	215623.196573	37.167501
1700.668100	216014.242799	37.172519
1702.692167	216402.290698	37.177536
1704.606736	216791.653532	37.182554
1706.222532	217178.044908	37.187572
1707.955079	217566.272573	37.192589
1709.440282	217959.850829	37.197607
1711.344488	218352.015306	37.202624
1713.493343	218749.525345	37.207642
1714.901162	219131.513864	37.212660
1717.080032	219521.529374	37.217677
1718.566505	219911.863897	37.222695
1720.528342	220302.324534	37.227712
1722.059037	220681.479128	37.232730
1723.967021	221073.754788	37.237748
1725.588240	221469.558895	37.242765
1727.554822	221856.239894	37.247783
1729.395578	222247.184688	37.252800
1730.860787	222645.609468	37.257818
1732.429364	223028.931335	37.262836
1734.573629	223412.464186	37.267853
1736.394847	223808.599043	37.272871
1738.351012	224197.169253	37.277888
1739.743566	224639.554251	37.282906
1741.655840	225033.061976	37.287924
1743.196330	225408.446055	37.292941
1745.094716	225801.272746	37.297959
1746.887736	226185.126459	37.302976
1748.493541	226572.161880	37.307994
1749.912893	226958.213262	37.313012
1752.499942	227342.117109	37.318029
1753.735556	227728.658332	37.323047
1755.198752	228103.072490	37.328064
1757.095093	228483.207466	37.333082
1758.693795	228851.428999	37.338100
1760.643865	229210.982671	37.343117
1762.334416	229583.229684	37.348135
1763.819131	229946.570608	37.353152
1765.664752	230322.985077	37.358170
1767.551936	230696.091545	37.363188
1769.457143	231067.189311	37.368205
1770.972165	231448.970077	37.373223
1772.409060	231825.455888	37.378240
1774.146703	232211.824803	37.383258
1775.902946	232593.695595	37.388276
1777.240415	232982.113805	37.393293
1778.769286	233383.659241	37.398311
1780.699814	233774.242131	37.403328
1782.673896	234179.805616	37.408346
1784.307306	234593.275420	37.413364
1786.186256	234993.598457	37.418381
1787.890558	235407.591945	37.423399
1789.516310	235813.801055	37.428416
1791.657674	236224.879270	37.433434
1793.002854	236638.985713	37.438452
1795.243839	237051.649631	37.443469
1796.710365	237491.139780	37.448487
1798.643911	237898.293274	37.453504
1800.504802	238314.299515	37.458522
1802.497347	238743.163728	37.463540
1804.309760	239158.062005	37.468557
1806.031142	239588.750894	37.473575
1807.934039	240009.427586	37.478592
1809.902696	240438.273758	37.483610
1811.576107	240869.430315	37.488628
1813.457442	241284.422826	37.493645
1815.225310	241728.418974	37.498663
1817.116458	242161.624925	37.503680
1819.042320	242595.918204	37.508698
1820.804244	243027.063977	37.513716
1822.775196	243454.136921	37.518733
1824.782240	243880.696527	37.523751
1826.542077	244317.814323	37.528768
1828.465866	244745.125662	37.533786
1830.204878	245187.023912	37.538804
1832.609062	245617.229277	37.543821
1834.065223	246053.815485	37.548839
1836.207450	246483.099967	37.553856
1838.137603	246912.013571	37.558874
1839.550952	247349.548429	37.563892
1841.656804	247779.653398	37.568909
1843.296415	248217.177314	37.573927
1845.012539	248653.647555	37.578944
1846.969148	249091.196277	37.583962
1848.855495	249539.705763	37.588980
1851.029533	249967.972734	37.593997
1852.568313	250409.325986	37.599015
1854.869636	250845.701701	37.604032
1856.795331	251279.421672	37.609050
1858.145697	251717.784155	37.614068
1860.297348	252152.127948	37.619085
1862.125201	252593.104938	37.624103
1864.077801	253031.445079	37.629120
1866.061576	253471.533156	37.634138
1867.705982	253919.450909	37.639156
1869.677785	254351.107548	37.644173
1871.344508	254792.290178	37.649191
1872.860104	255225.216477	37.654208
1875.098017	255673.697470	37.659226
1876.898486	256114.731471	37.664244
1878.766572	256545.440686	37.669261
1880.645257	256966.901441	37.674279
1882.264394	257384.747051	37.679296
1884.247213	257798.290301	37.684314
1885.875755	258229.852226	37.689332
1887.933080	258648.159042	37.694349
1889.531841	259075.839189	37.699367
1891.375949	259504.545736	37.704384
1893.748951	259931.488285	37.709402
1895.255168	260363.883197	37.714420
1897.408228	260794.926450	37.719437
1899.703466	261219.595302	37.724455
1901.290440	261653.526175	37.729472
1903.296522	262075.168724	37.734490
1905.130490	262530.117809	37.739508
1906.860431	262955.768526	37.744525
1908.701425	263397.684183	37.749543
1910.423119	263838.399953	37.754560
1912.997943	264285.909670	37.759578
1914.610576	264721.079624	37.764596
1916.494159	265168.550492	37.769613
1918.186514	265621.158646	37.774631
1920.101934	266074.263077	37.779648
1922.399503	266521.639134	37.784666
1924.278635	266976.577807	37.789684
1926.207255	267432.676422	37.794701
1928.236588	267893.025664	37.799719
1930.207427	268353.358679	37.804736
1932.106691	268805.218409	37.809754
1933.826848	269276.896099	37.814772
1935.867218	269730.814497	37.819789
1938.017501	270188.854853	37.824807
1939.746956	270667.692826	37.829824
1942.025757	271120.630151	37.834842
1943.728716	271586.083888	37.839860
1946.177842	272049.965769	37.844877
1947.999405	272519.285131	37.849895
1949.533374	272992.385418	37.854912
1951.637480	273462.901317	37.859930
1953.896044	273928.716831	37.864948
1955.882476	274401.993999	37.869965
1957.613475	274867.056671	37.874983
1959.499380	275345.530787	37.880000
1961.920843	275816.599646	37.885018
1963.839408	276290.494056	37.890036
1965.795633	276752.874042	37.895053
1967.937594	277232.521321	37.900071
1969.686329	277714.671083	37.905088
1971.862403	278177.900832	37.910106
1973.724988	278659.445385	37.915124
1975.883583	279132.430256	37.920141
1977.927273	279601.444869	37.925159
1979.916572	280080.577271	37.930176
1982.170998	280546.201734	37.935194
1984.054651	281021.411900	37.940212
1986.099681	281493.901602	37.945229
1987.996818	281955.542583	37.950247
1989.803265	282437.543946	37.955264
1991.990168	282906.983614	37.960282
1994.069383	283387.286141	37.965300
1996.020329	283852.494663	37.970317
1997.528346	284334.234980	37.975335
1999.730180	284807.299085	37.980352
2001.942776	285274.517724	37.985370
2004.302762	285747.578233	37.990388
2006.004007	286225.800800	37.995405
2008.274726	286692.624417	38.000423
2010.036463	287166.668184	38.005440
2011.843942	287626.402243	38.010458
2013.742687	288092.673082	38.015476
2015.688431	288533.534080	38.020493
2017.618077	288980.263808	38.025511
2019.906105	289437.524821	38.030528
2021.920978	289891.527319	38.035546
2023.873076	290353.438050	38.040564
2025.789482	290816.038815	38.045581
2027.712804	291267.232158	38.050599
2029.207916	291728.832321	38.055616
2031.464084	292201.150810	38.060634
2033.166074	292668.021826	38.065652
2034.949897	293143.310172	38.070669
2036.757539	293632.105197	38.075687
2038.621746	294120.711035	38.080704
2040.556315	294618.497709	38.085722
2042.137574	295115.426158	38.090740
2044.311699	295624.623843	38.095757
2046.466149	296132.120696	38.100775
2048.486786	296646.825130	38.105792
2050.623845	297155.666176	38.110810
2052.601626	297679.211432	38.115828
2054.548251	298204.638688	38.120845
2057.126267	298721.831571	38.125863
2059.120233	299237.060996	38.130880
2061.078475	299759.557509	38.135898
2063.233212	300282.755366	38.140916
2065.271520	300821.513072	38.145933
2067.566785	301324.998862	38.150951
2069.513621	301870.369164	38.155968
2071.634492	302397.040544	38.160986
2073.978730	302933.373793	38.166004
2076.039148	303465.839628	38.171021
2078.141306	304000.911333	38.176039
2080.147140	304535.437025	38.181056
2082.411246	305071.643828	38.186074
2084.499616	305609.425548	38.191092
2086.857706	306141.648418	38.196109
2088.883764	306662.519949	38.201127
2090.753987	307211.552719	38.206144
2092.999001	307745.942846	38.211162
2095.511582	308292.195904	38.216180
2097.578660	308831.611310	38.221197
2099.825726	309368.225335	38.226215
2101.877841	309908.042347	38.231232
2104.032119	310445.248544	38.236250
2106.148075	310974.432654	38.241268
2108.340587	311519.700697	38.246285
2110.240092	312062.245262	38.251303
2112.230743	312594.079954	38.256320
2114.451718	313148.295818	38.261338
2116.667540	313689.862286	38.266356
2118.926201	314244.343096	38.271373
2121.139178	314770.056445	38.276391
2123.244835	315313.787547	38.281408
2125.258921	315861.440191	38.286426
2127.453483	316420.053954	38.291444
2129.366735	316968.908152	38.296461
2131.878356	317500.798641	38.301479
2133.810723	318057.614336	38.306496
2135.970257	318595.927959	38.311514
2138.485709	319151.267306	38.316532
2139.961878	319695.296596	38.321549
2142.499172	320232.189021	38.326567
2144.412833	320790.356351	38.331584
2146.649631	321337.293527	38.336602
2148.809044	321888.047500	38.341620
2150.741082	322441.043281	38.346637
2153.069628	322981.349795	38.351655
2155.302812	323510.064127	38.356672
2157.104985	324026.277120	38.361690
2159.380967	324551.471770	38.366708
2161.325602	325088.192726	38.371725
2163.804683	325614.588868	38.376743
2165.422627	326134.724549	38.381760
2167.466741	326664.966342	38.386778
2169.563830	327193.671378	38.391796
2171.774226	327732.025998	38.396813
2173.561061	328266.155014	38.401831
2175.626580	328827.322102	38.406848
2177.793986	329373.843628	38.411866
2179.779455	329931.255836	38.416884
2181.868275	330493.697602	38.421901
2183.925429	331063.932813	38.426919
2186.046477	331645.829576	38.431936
2188.290641	332215.666782	38.436954
2190.994674	332789.915567	38.441972
2192.763881	333372.309214	38.446989
2194.874319	333942.937540	38.452007
2196.890877	334537.894516	38.457024
2198.934225	335125.758040	38.462042
2201.139655	335718.081431	38.467060
2203.499121	336331.188046	38.472077
2205.898390	336926.791209	38.477095
2207.674333	337537.340027	38.482112
2209.976444	338137.565183	38.487130
2212.667533	338740.866634	38.492148
2214.837554	339358.004521	38.497165
2216.946608	339960.905234	38.502183
2219.081487	340580.242214	38.507200
2221.043210	341200.006170	38.512218
2223.496805	341810.086855	38.517236
2225.948494	342444.374133	38.522253
2228.597485	343057.376593	38.527271
2230.567297	343684.975784	38.532288
2232.786876	344308.439277	38.537306
2235.205132	344931.811040	38.542324
2237.297431	345555.812104	38.547341
2239.663280	346177.323283	38.552359
2242.080095	346813.486857	38.557376
2243.978990	347452.341159	38.562394
2246.935458	348075.708848	38.567412
2249.024373	348702.687979	38.572429
2251.186698	349334.797969	38.577447
2253.477910	349957.412047	38.582464
2255.823855	350585.743591	38.587482
2258.193584	351217.056733	38.592500
2260.492879	351847.890288	38.597517
2262.777329	352475.088435	38.602535
2265.169690	353117.155120	38.607552
2267.358920	353745.670078	38.612570
2269.732482	354368.892811	38.617588
2271.560836	355008.207623	38.622605
2274.286365	355638.483793	38.627623
2276.891669	356272.348015	38.632640
2279.171638	356902.627925	38.637658
2281.450470	357528.382068	38.642676
2283.269576	358173.308021	38.647693
2285.621534	358798.396414	38.652711
2288.151870	359424.181529	38.657728
2290.093429	360072.888248	38.662746
2292.439007	360701.677802	38.667764
2294.629045	361334.491641	38.672781
2297.248933	361966.970733	38.677799
2299.553910	362608.548596	38.682816
2301.836932	363254.102531	38.687834
2304.148392	363863.338315	38.692852
2306.479406	364490.547469	38.697869
2308.508884	365087.709718	38.702887
2310.807247	365690.602076	38.707904
2312.791378	366308.300433	38.712922
2315.678556	366915.692951	38.717940
2317.701913	367522.178187	38.722957
2319.981711	368131.274683	38.727975
2322.218956	368747.977875	38.732992
2324.317421	369363.881993	38.738010
2326.987907	369970.194994	38.743028
2328.863771	370600.192462	38.748045
2331.185248	371224.779067	38.753063
2333.622961	371857.198336	38.758080
2335.977057	372489.899262	38.763098
2338.323643	373128.702575	38.768116
2340.788503	373769.833548	38.773133
2342.738243	374399.473029	38.778151
2345.324791	375038.633350	38.783168
2347.542893	375688.367437	38.788186
2349.912450	376342.324882	38.793204
2352.025367	377001.764626	38.798221
2354.670710	377655.626268	38.803239
2357.035661	378319.741213	38.808256
2359.253049	378978.694459	38.813274
2361.735227	379636.779710	38.818292
2363.900411	380309.028333	38.823309
2366.315993	380967.123801	38.828327
2368.551638	381650.896368	38.833344
2371.054993	382329.564838	38.838362
2373.951007	382998.975946	38.843380
2376.643258	383681.160323	38.848397
2378.415995	384354.430723	38.853415
2381.108126	385033.290638	38.858432
2383.227711	385713.143407	38.863450
2385.928020	386381.857578	38.868468
2388.345227	387072.863386	38.873485
2390.897995	387748.316704	38.878503
2393.201138	388437.384751	38.883520
2395.663120	389136.627567	38.888538
2398.130010	389811.188634	38.893556
2400.584464	390509.514538	38.898573
2403.022389	391190.235451	38.903591
2405.866297	391877.870295	38.908608
2407.942383	392563.791315	38.913626
2410.689454	393244.744857	38.918644
2412.879321	393937.510296	38.923661
2415.303556	394615.520583	38.928679
2417.916050	395312.569273	38.933696
2419.930508	396002.020910	38.938714
2422.333163	396698.032519	38.943732
2424.746270	397399.956265	38.948749
2427.182302	398102.974471	38.953767
2429.960513	398799.304956	38.958784
2432.426116	399504.590479	38.963802
2434.761840	400196.348163	38.968820
2437.697284	400893.869138	38.973837
2439.852272	401596.620443	38.978855
2442.452050	402281.923757	38.983872
2444.758544	402983.272696	38.988890
2447.329008	403672.347796	38.993908
2449.356699	404372.213086	38.998925
2451.828328	405080.880640	39.003943
2454.387478	405774.998205	39.008960
2456.800155	406481.030004	39.013978
2459.222589	407181.569773	39.018996
2461.811117	407886.902941	39.024013
2464.088230	408588.114544	39.029031
2466.785444	409271.353863	39.034048
2469.154049	409954.174093	39.039066
2471.446765	410622.221307	39.044084
2473.929115	411289.029969	39.049101
2475.853719	411965.868624	39.054119
2478.511375	412631.044145	39.059136
2480.614332	413320.230040	39.064154
2483.047834	414007.722286	39.069172
2485.379581	414687.893596	39.074189
2488.260270	415390.345350	39.079207
2490.557611	416075.348663	39.084224
2492.731437	416790.845853	39.089242
2495.235063	417487.199212	39.094260
2497.426203	418202.805999	39.099277
2500.057508	418917.762897	39.104295
2502.484777	419631.416476	39.109312
2504.733706	420358.246574	39.114330
2507.202269	421085.880273	39.119348
2509.532350	421825.390813	39.124365
2512.051917	422554.568341	39.129383
2514.586795	423303.850262	39.134400
2517.131472	424056.652271	39.139418
2519.915547	424806.100408	39.144436
2522.177807	425558.193875	39.149453
2524.613638	426320.361658	39.154471
2527.424710	427078.038706	39.159488
2529.972971	427841.000559	39.164506
2532.170187	428611.589979	39.169524
2535.073786	429371.811728	39.174541
2537.959434	430145.072852	39.179559
2540.321869	430904.879024	39.184576
2542.748174	431682.468296	39.189594
2545.521701	432457.595389	39.194612
2548.165645	433221.531817	39.199629
2550.889761	434011.445864	39.204647
2553.758552	434782.734013	39.209664
2556.543102	435563.525108	39.214682
2558.716951	436332.294598	39.219700
2561.521175	437117.280508	39.224717
2563.849698	437897.358315	39.229735
2567.124166	438667.435847	39.234752
2569.520398	439455.697035	39.239770
2572.139561	440234.886717	39.244788
2574.695607	441011.630801	39.249805
2577.231862	441793.815463	39.254823
2579.752577	442566.412425	39.259840
2582.211508	443348.301691	39.264858
2584.618069	444139.632372	39.269876
2587.767433	444920.845536	39.274893
2590.422668	445720.273287	39.279911
2592.935900	446498.752122	39.284928
2595.586253	447290.180414	39.289946
2598.025820	448084.193967	39.294964
2600.904669	448872.035809	39.299981
2603.254183	449657.811442	39.304999
2605.994321	450448.298276	39.310016
2608.454051	451246.236254	39.315034
2611.080320	452040.272848	39.320052
2613.804870	452840.685604	39.325069
2616.065532	453637.654805	39.330087
2618.874424	454431.620571	39.335104
2621.224608	455244.896878	39.340122
2624.077478	456041.574394	39.345140
2626.650627	456841.705210	39.350157
2629.181386	457648.131529	39.355175
2631.818119	458449.452574	39.360192
2634.621185	459257.438276	39.365210
2636.964641	460058.490985	39.370228
2639.853486	460852.041209	39.375245
2642.328071	461631.828230	39.380263
2645.346338	462395.875819	39.385280
2647.870142	463156.336217	39.390298
2650.531359	463930.997926	39.395316
2653.190409	464694.763023	39.400333
2655.490752	465482.715417	39.405351
2658.023025	466250.079487	39.410368
2660.459655	467028.243635	39.415386
2662.947783	467819.203511	39.420404
2666.053556	468596.233984	39.425421
2668.493663	469391.230212	39.430439
2671.219323	470170.482861	39.435456
2673.698964	470973.794214	39.440474
2676.238139	471771.251617	39.445492
2679.133946	472576.093663	39.450509
2681.606047	473384.406487	39.455527
2683.832173	474194.796254	39.460544
2686.617034	475017.081140	39.465562
2689.205712	475847.696565	39.470580
2691.936944	476674.412544	39.475597
2694.313897	477516.706280	39.480615
2696.850412	478350.399783	39.485632
2699.238516	479203.977979	39.490650
2701.983348	480062.759988	39.495668
2704.662131	480918.280467	39.500685
2707.242474	481799.832532	39.505703
2709.962728	482658.495544	39.510720
2712.776265	483540.125924	39.515738
2715.406314	484425.883177	39.520756
2718.404214	485301.842495	39.525773
2720.492872	486202.645332	39.530791
2724.046373	487093.619851	39.535808
2726.681588	487968.648723	39.540826
2729.484601	488879.241998	39.545844
2732.289409	489762.077911	39.550861
2734.660665	490661.141527	39.555879
2737.505957	491572.142105	39.560896
2740.391383	492473.499644	39.565914
2743.011221	493386.106844	39.570932
2746.186095	494282.830461	39.575949
2748.756261	495204.229686	39.580967
2751.620430	496112.059178	39.585984
2754.486830	497032.654294	39.591002
2757.340179	497946.037562	39.596020
2760.234853	498848.467983	39.601037
2763.033351	499770.387130	39.606055
2765.793947	500680.256673	39.611072
2768.705679	501592.472415	39.616090
2771.362315	502518.297317	39.621108
2774.515878	503425.126604	39.626125
2777.330036	504345.022918	39.631143
2780.427424	505248.785111	39.636160
2783.291531	506163.578377	39.641178
2785.789452	507072.128243	39.646196
2789.217901	507991.313409	39.651213
2791.786543	508903.983486	39.656231
2794.191740	509806.646941	39.661248
2797.398216	510714.722678	39.666266
2800.319180	511633.782282	39.671284
2803.218075	512524.415024	39.676301
2806.172892	513433.737395	39.681319
2808.955729	514347.117799	39.686336
2812.191201	515243.740031	39.691354
2814.661436	516141.545614	39.696372
2817.940506	517045.313488	39.701389
2820.615017	517941.671235	39.706407
2823.137953	518841.629574	39.711424
2826.059578	519715.926745	39.716442
2828.931485	520603.028539	39.721460
2831.804739	521447.461743	39.726477
2834.290966	522315.435609	39.731495
2837.017852	523172.037541	39.736512
2839.768466	524031.709771	39.741530
2842.359901	524893.827049	39.746548
2845.427055	525760.147416	39.751565
2848.350539	526627.649950	39.756583
2850.776429	527503.794741	39.761600
2853.498278	528383.464447	39.766618
2856.312000	529272.481974	39.771636
2859.371202	530148.567467	39.776653
2861.856951	531044.177911	39.781671
2864.721223	531927.942241	39.786688
2867.630440	532837.166232	39.791706
2870.017318	533748.785305	39.796724
2873.167622	534657.855787	39.801741
2875.424011	535579.749246	39.806759
2878.503929	536503.159006	39.811776
2881.163683	537426.327141	39.816794
2883.807278	538378.119102	39.821812
2886.533957	539304.727461	39.826829
2889.633672	540265.877719	39.831847
2892.460845	541221.524318	39.836864
2895.503260	542188.389036	39.841882
2898.375130	543148.726781	39.846900
2901.580954	544118.801813	39.851917
2904.349087	545090.440769	39.856935
2907.360239	546065.642997	39.861952
2910.433843	547026.183495	39.866970
2913.131146	548016.637328	39.871988
2915.943335	548995.587769	39.877005
2918.950296	549981.273721	39.882023
2921.790110	550976.668893	39.887040
2924.911061	551953.144878	39.892058
2927.609785	552964.956004	39.897076
2930.482981	553956.809898	39.902093
2933.314556	554965.232689	39.907111
2936.367946	555975.653874	39.912128
2939.796716	556978.148327	39.917146
2942.141667	557998.834479	39.922164
2945.440501	559001.499560	39.927181
2948.353586	560026.859771	39.932199
2951.328339	561046.554256	39.937216
2954.269623	562058.289158	39.942234
2957.384301	563078.706933	39.947252
2960.433369	564098.955383	39.952269
2963.702158	565123.305962	39.957287
2966.242964	566144.080275	39.962304
2969.626857	567165.388138	39.967322
2972.458206	568207.591847	39.972340
2975.855031	569229.838134	39.977357
2978.371224	570249.788617	39.982375
2981.302249	571286.755437	39.987392
2984.604323	572316.499668	39.992410
2987.042927	573359.601716	39.997428
2989.874628	574388.050239	40.002445
2992.882139	575430.184446	40.007463
2996.128544	576479.267001	40.012480
2999.225305	577510.626563	40.017498
3002.538373	578554.757336	40.022516
3005.497621	579598.507380	40.027533
3008.145493	580640.715901	40.032551
3011.277482	581686.367352	40.037568
3014.618399	582721.564787	40.042586
3017.305778	583773.229440	40.047604
3020.293609	584822.096436	40.052621
3023.297717	585846.404307	40.057639
3026.378547	586864.697422	40.062656
3029.307539	587853.104284	40.067674
3032.357123	588866.972510	40.072692
3035.272060	589860.629646	40.077709
3038.136319	590868.144226	40.082727
3040.758858	591884.783528	40.087744
3044.194044	592890.679645	40.092762
3046.642538	593909.829545	40.097780
3049.981056	594929.696510	40.102797
3053.107870	595956.422669	40.107815
3055.546063	596987.379802	40.112832
3058.807177	598031.933372	40.117850
3061.787042	599080.495997	40.122868
3064.802704	600124.150820	40.127885
3067.773301	601182.089000	40.132903
3070.572877	602248.068884	40.137920
3073.743634	603306.279463	40.142938
3076.680046	604382.200799	40.147956
3079.949442	605455.613419	40.152973
3083.039421	606537.111925	40.157991
3085.533993	607617.904853	40.163008
3089.039471	608704.432220	40.168026
3092.037315	609804.797343	40.173044
3095.012941	610903.507436	40.178061
3098.209366	612018.780656	40.183079
3101.210135	613139.576502	40.188096
3104.469752	614248.063701	40.193114
3107.255543	615383.271846	40.198132
3110.635801	616500.314572	40.203149
3113.311761	617627.759310	40.208167
3116.664836	618769.973987	40.213184
3119.823341	619907.102693	40.218202
3122.794227	621058.987975	40.223220
3125.850955	622207.688325	40.228237
3128.872863	623358.221263	40.233255
3131.787834	624528.834914	40.238272
3135.349807	625686.025006	40.243290
3138.393011	626872.248833	40.248308
3141.588315	628036.188464	40.253325
3145.186665	629202.381440	40.258343
3147.960597	630381.465845	40.263360
3151.667866	631552.924739	40.268378
3154.525190	632738.522493	40.273396
3157.855517	633917.618235	40.278413
3161.176257	635082.107127	40.283431
3164.119476	636266.641620	40.288448
3167.519694	637451.414761	40.293466
3170.870678	638637.756867	40.298484
3173.821824	639823.629237	40.303501
3177.080234	641009.364000	40.308519
3180.049816	642202.640845	40.313536
3183.687041	643387.937522	40.318554
3186.833714	644582.053636	40.323572
3189.946332	645769.353045	40.328589
3193.110120	646948.178323	40.333607
3196.085078	648139.409484	40.338624
3199.846395	649340.936923	40.343642
3202.832439	650548.129528	40.348660
3206.016915	651739.993876	40.353677
3209.309211	652924.073879	40.358695
3212.582121	654121.716463	40.363712
3215.990744	655320.386952	40.368730
3219.268217	656526.005961	40.373748
3222.237987	657720.819757	40.378765
3225.600178	658906.957295	40.383783
3228.675521	660120.283248	40.388800
3232.003127	661297.272159	40.393818
3234.903029	662487.479417	40.398836
3238.181412	663648.211054	40.403853
3241.282159	664806.592369	40.408871
3244.380392	665976.378663	40.413888
3247.541307	667127.751447	40.418906
3250.624955	668295.464669	40.423924
3253.495456	669453.767591	40.428941
3256.717430	670620.972681	40.433959
3259.915970	671794.850352	40.438976
3262.833177	672973.799248	40.443994
3266.053090	674154.240489	40.449012
3269.040872	675361.166594	40.454029
3272.485962	676563.437315	40.459047
3275.608384	677764.412870	40.464064
3278.577986	678978.078433	40.469082
3281.767764	680203.472678	40.474100
3285.288407	681439.826945	40.479117
3288.700390	682668.830024	40.484135
3291.550146	683906.402335	40.489152
3294.551126	685149.889696	40.494170
3298.136665	686403.636684	40.499188
3301.504659	687668.564929	40.504205
3304.889998	688928.498168	40.509223
3308.100315	690195.033583	40.514240
3311.321338	691455.234994	40.519258
3314.746718	692745.689715	40.524276
3317.969027	694033.163227	40.529293
3321.601116	695302.624897	40.534311
3325.149423	696597.310996	40.539328
3328.430784	697889.768369	40.544346
3331.947952	699184.723820	40.549364
3335.319863	700482.486236	40.554381
3339.206222	701758.657741	40.559399
3342.325542	703050.775991	40.564416
3345.932898	704360.360730	40.569434
3349.535732	705643.093466	40.574452
3352.901785	706942.615770	40.579469
3356.718036	708236.270628	40.584487
3360.188177	709529.737614	40.589504
3363.619646	710818.459760	40.594522
3367.038235	712114.464336	40.599540
3369.973552	713404.806721	40.604557
3373.668142	714701.557915	40.609575
3377.107330	716009.730824	40.614592
3380.558057	717297.957347	40.619610
3383.921732	718611.426688	40.624628
3387.067641	719902.369228	40.629645
3390.781642	721195.836728	40.634663
3394.205750	722515.504443	40.639680
3397.594210	723804.662570	40.644698
3400.961567	725095.649182	40.649716
3404.303199	726402.301536	40.654733
3407.873375	727707.324240	40.659751
3411.422669	729011.894799	40.664768
3414.920240	730331.479304	40.669786
3418.582447	731620.595593	40.674804
3421.895413	732948.575614	40.679821
3425.644569	734240.419806	40.684839
3429.014676	735546.583016	40.689856
3432.198412	736838.891967	40.694874
3436.002006	738138.588314	40.699892
3439.006477	739445.802843	40.704909
3442.707283	740741.291398	40.709927
3446.179494	742047.161225	40.714944
3449.408408	743345.605406	40.719962
3453.426283	744639.612632	40.724980
3456.466960	745939.828576	40.729997
3459.999809	747242.655510	40.735015
3463.356761	748519.433899	40.740020
3467.018983	749756.865498	40.745024
3470.129586	750939.954544	40.750029
3473.436613	752053.835160	40.755034
3476.923564	753103.922137	40.760039
3480.087852	754098.569632	40.765044
3482.782112	755001.043182	40.770048
3485.829113	755853.840563	40.775053
3488.187741	756637.899866	40.780058
3490.680077	757350.737697	40.785063
3493.495312	757996.734877	40.790068
3495.651808	758581.942252	40.795072
3498.024073	759096.361203	40.800077
3499.689783	759563.594412	40.805082
3502.089852	759968.365406	40.810087
3503.676811	760335.803818	40.815092
3505.414454	760627.178207	40.820096
3507.337689	760878.454046	40.825101
3508.904446	761090.711237	40.830106
3510.123078	761244.417565	40.835111
3511.151690	761361.994793	40.840116
3512.363946	761434.898734	40.845120
3513.878551	761467.846540	40.850125
3514.552171	761473.901520	40.855130
3515.520387	761449.127762	40.860135
3516.370824	761401.583991	40.865140
3517.007859	761314.119335	40.870144
3517.907816	761198.739532	40.875149
3518.260373	761075.160764	40.880154
3519.325534	760920.186912	40.885159
3519.893798	760748.765590	40.890164
3520.502856	760552.124446	40.895168
3521.063781	760340.537768	40.900173
3521.084548	760103.231432	40.905178
3521.558696	759856.518135	40.910183
3521.840960	759595.421326	40.915188
3522.212215	759325.912870	40.920192
3522.742979	759049.608576	40.925197
3523.109030	758758.912683	40.930202
3523.356828	758441.577861	40.935207
3523.518071	758119.161106	40.940212
3523.713516	757802.745883	40.945216
3524.107888	757452.477774	40.950221
3523.925370	757117.440768	40.955226
3524.218991	756763.998866	40.960231
3524.338674	756421.576542	40.965236
3524.159378	756055.198049	40.970240
3524.494207	755692.567727	40.975245
3524.307968	755317.763029	40.980250
3524.431003	754946.739845	40.985255
3524.568275	754579.300497	40.990260
3524.377155	754193.925401	40.995264
3524.528669	753805.561264	41.000269
3524.500947	753429.058063	41.005274
3524.273807	753036.520210	41.010279
3524.403807	752646.125782	41.015284
3524.295237	752261.776064	41.020288
3524.586431	751872.155446	41.025293
3523.938257	751481.188178	41.030298
3524.107431	751091.548268	41.035303
3523.947489	750700.757425	41.040308
3523.708128	750317.271013	41.045312
3523.862130	749917.299430	41.050317
3523.862067	749525.681919	41.055322
3523.863629	749143.036394	41.060327
3523.630706	748737.385966	41.065332
3523.319735	748348.724879	41.070336
3523.673447	747953.560421	41.075341
3523.178021	747573.241998	41.080346
3522.951979	747175.465095	41.085351
3523.065231	746794.118832	41.090356
3523.025634	746403.932229	41.095360
3523.211725	746021.004082	41.100365
3522.478697	745638.752348	41.105370
3522.644912	745242.493000	41.110375
3522.526580	744857.926891	41.115380
3522.308294	744477.807655	41.120384
3522.089082	744090.600440	41.125389
3521.626805	743719.531968	41.130394
3521.713894	743343.856123	41.135399
3521.628022	742968.586414	41.140404
3521.200057	742601.069087	41.145408
3521.359871	742223.003759	41.150413
3521.028372	741868.738555	41.155418
3521.138101	741502.861780	41.160423
3520.706973	741140.469734	41.165428
3520.284718	740776.724218	41.170432
3520.692822	740420.986352	41.175437
3520.398828	740069.354779	41.180442
3520.159173	739710.526085	41.185447
3519.772951	739357.196300	41.190452
3519.495708	739011.550233	41.195456
3519.725923	738664.667661	41.200461
3519.425822	738327.851242	41.205466
3519.335456	737974.757625	41.210471
3519.243191	737645.448073	41.215476
3518.789736	737313.314544	41.220480
3519.145983	736967.871288	41.225485
3518.728118	736628.528364	41.230490
3518.646149	736291.788007	41.235495
3518.496116	735973.900126	41.240500
3518.148088	735648.955004	41.245504
3518.371741	735320.833930	41.250509
3517.851911	734986.387548	41.255514
3517.885536	734677.030181	41.260519
3517.862760	734349.256488	41.265524
3517.413258	734043.815296	41.270528
3517.895745	733714.843481	41.275533
3517.239614	733418.372668	41.280538
3517.167119	733097.338374	41.285543
3517.188176	732793.306944	41.290548
3516.821738	732497.249617	41.295552
3516.736820	732181.973703	41.300557
3516.454846	731885.335395	41.305562
3516.270262	731593.027586	41.310567
3516.316915	731295.620284	41.315572
3516.224520	731002.780797	41.320576
3516.540602	730709.368212	41.325581
3516.107994	730421.466423	41.330586
3515.873319	730133.521806	41.335591
3515.908944	729828.980457	41.340596
3515.674984	729553.347365	41.345600
3515.463070	729263.585146	41.350605
3515.635665	728982.120189	41.355610
3515.342574	728703.644732	41.360615
3515.285091	728426.507932	41.365620
3514.802639	728154.038692	41.370624
3514.734831	727881.442493	41.375629
3514.466007	727621.404040	41.380634
3514.600214	727345.189757	41.385639
3514.640077	727077.998642	41.390644
3514.239322	726830.045404	41.395648
3514.198692	726555.468262	41.400653
3513.795986	726303.287914	41.405658
3514.033703	726044.007749	41.410663
3513.907864	725785.522567	41.415668
3513.571822	725534.249067	41.420672
3513.527560	725286.735497	41.425677
3513.291704	725035.876235	41.430682
3513.084032	724792.289626	41.435687
3512.947185	724563.551800	41.440692
3512.869035	724316.758009	41.445696
3513.103018	724069.013282	41.450701
3512.738584	723849.660310	41.455706
3512.421961	723600.654027	41.460711
3512.470954	723374.182110	41.465716
3512.494965	723144.734057	41.470720
3512.349707	722912.085553	41.475725
3512.096537	722693.674904	41.480730
3511.633812	722451.449144	41.485735
3511.827606	722250.551022	41.490740
3511.800417	722033.027581	41.495744
3511.915225	721809.724291	41.500749
3511.328025	721599.321433	41.505754
3511.511442	721389.976130	41.510759
3511.314344	721164.674169	41.515764
3510.973161	720957.139657	41.520768
3511.265686	720752.321699	41.525773
3510.751882	720542.425346	41.530778
3511.196502	720339.059635	41.535783
3511.043940	720125.324836	41.540788
3510.632450	719920.453636	41.545792
3510.661126	719719.868599	41.550797
3510.296517	719536.402142	41.555802
3510.466580	719322.791941	41.560807
3510.455139	719122.893410	41.565812
3510.293054	718942.207216	41.570816
3510.327962	718748.838290	41.575821
3510.035605	718561.073422	41.580826
3509.943224	718366.228769	41.585831
3509.791058	718184.235048	41.590836
3509.749123	717999.838497	41.595840
3509.833918	717816.458582	41.600845
3509.436722	717636.973283	41.605850
3509.476352	717458.007375	41.610855
3509.653408	717278.221364	41.615860
3508.999703	717094.798522	41.620864
3509.328553	716926.388731	41.625869
3509.177180	716756.913764	41.630874
3508.824774	716580.771628	41.635879
3509.206302	716406.687595	41.640884
3508.589597	716242.983781	41.645888
3508.547999	716067.226136	41.650893
3508.595536	715920.373014	41.655898
3508.533279	715760.239602	41.660903
3508.938152	715590.302169	41.665908
3508.270926	715428.029560	41.670912
3508.726316	715265.816919	41.675917
3508.192172	715110.611091	41.680922
3508.311545	714951.920830	41.685927
3508.348950	714789.718281	41.690932
3508.071771	714631.881209	41.695936
3507.916092	714474.815064	41.700941
3507.973299	714337.806908	41.705946
3507.877557	714184.645441	41.710951
3507.751999	714031.585351	41.715956
3507.834042	713881.118266	41.720960
3508.019700	713732.715606	41.725965
3507.718224	713586.871811	41.730970
3507.908318	713436.974509	41.735975
3508.005963	713285.402506	41.740980
3507.609088	713149.541679	41.745984
3507.548241	712984.988221	41.750989
3507.592913	712856.196305	41.755994
3507.294595	712711.776130	41.760999
3507.413221	712569.567776	41.766004
3507.320438	712434.786868	41.771008
3507.497574	712276.433924	41.776013
3506.967058	712143.507255	41.781018
3506.891779	712013.233325	41.786023
3507.096274	711880.379959	41.791028
3506.843886	711753.903421	41.796032
3506.906623	711614.070739	41.801037
3506.430453	711486.336562	41.806042
3506.372485	711350.738526	41.811047
3506.446307	711235.914891	41.816052
3506.328774	711104.343405	41.821056
3506.411961	710982.515762	41.826061
3506.162056	710876.774972	41.831066
3506.249313	710737.023112	41.836071
3506.168119	710615.713714	41.841076
3506.003916	710497.047300	41.846080
3506.001502	710378.849003	41.851085
3505.831467	710285.349480	41.856090
3506.027916	710156.193780	41.861095
3505.740488	710041.661792	41.866100
3505.276798	709922.788506	41.871104
3505.767368	709826.792124	41.876109
3505.527269	709720.241032	41.881114
3505.367501	709618.044332	41.886119
3505.518803	709497.524725	41.891124
3505.184558	709408.858504	41.896128
3505.142249	709295.914520	41.901133
3505.038160	709198.519591	41.906138
3505.215029	709098.048592	41.911143
3505.574317	708989.651867	41.916148
3505.427370	708888.933863	41.921152
3505.711407	708787.100966	41.926157
3505.272313	708692.039465	41.931162
3505.171028	708575.371736	41.936167
3505.559645	708461.402320	41.941172
3505.342598	708364.016505	41.946176
3505.316438	708257.958139	41.951181
3505.402242	708157.640078	41.956186
3505.105605	708062.945364	41.961191
3505.351449	707953.660413	41.966196
3505.053798	707860.502994	41.971200
3505.338653	707758.409455	41.976205
3504.970029	707661.090287	41.981210
3505.165886	707561.243706	41.986215
3504.996111	707464.088175	41.991220
3504.805081	707380.194340	41.996224
3505.050270	707262.756420	42.001229
3504.545506	707178.366036	42.006234
3504.532060	707087.338496	42.011239
3504.531934	706990.497289	42.016244
3504.435322	706907.576529	42.021248
3504.670798	706815.958808	42.026253
3504.829636	706731.703012	42.031258
3504.345642	706645.565732	42.036263
3504.487660	706547.603499	42.041268
3504.694467	706466.764092	42.046272
3504.726998	706374.330798	42.051277
3504.118066	706285.131199	42.056282
3504.277172	706207.326876	42.061287
3504.346825	706120.050102	42.066292
3504.172292	706023.574424	42.071296
3504.479446	705938.640747	42.076301
3504.143910	705861.411490	42.081306
3504.294162	705772.528510	42.086311
3504.172594	705690.841881	42.091316
3503.802332	705619.526903	42.096320
3504.171345	705547.990183	42.101325
3504.010268	705456.274335	42.106330
3503.883157	705382.334421	42.111335
3503.893241	705293.866980	42.116340
3503.918646	705220.397272	42.121344
3503.920173	705142.609312	42.126349
3504.086103	705076.019785	42.131354
3503.579816	704997.867132	42.136359
3503.868704	704917.744796	42.141364
3503.933977	704840.042958	42.146368
3504.098302	704762.820853	42.151373
3503.826379	704697.641790	42.156378
3503.861602	704628.238836	42.161383
3503.940969	704537.020046	42.166388
3503.801331	704474.549717	42.171392
3503.760673	704389.807155	42.176397
3503.897522	704318.944329	42.181402
3503.584770	704242.143931	42.186407
3503.655325	704167.217164	42.191412
3503.592068	704086.996124	42.196416
3503.637496	704018.133068	42.201421
3503.525197	703954.412489	42.206426
3503.486281	703886.953326	42.211431
3503.755866	703821.380353	42.216436
3503.207745	703764.486763	42.221440
3503.530870	703671.678581	42.226445
3503.472223	703610.927530	42.231450
3503.516685	703547.774315	42.236455
3503.441342	703469.536842	42.241460
3503.530329	703401.953464	42.246464
3503.403499	703330.529806	42.251469
3503.377170	703267.187478	42.256474
3503.200755	703201.981416	42.261479
3503.479471	703133.023207	42.266484
3503.401604	703080.817368	42.271488
3503.481635	702997.084687	42.276493
3503.062957	702937.083837	42.281498
3503.310755	702878.065849	42.286503
3503.426917	702816.336396	42.291508
3502.826371	702748.414368	42.296512
3503.045683	702671.810507	42.301517
3502.801996	702613.169828	42.306522
3502.714952	702564.092715	42.311527
3503.181176	702500.713327	42.316532
3502.961587	702442.465031	42.321536
3502.952772	702383.287214	42.326541
3502.783301	702336.955293	42.331546
3502.655195	702278.243619	42.336551
3503.168917	702215.400913	42.341556
3502.888570	702152.539524	42.346560
3502.952211	702087.434612	42.351565
3502.838560	702043.725534	42.356570
3502.809413	701986.287548	42.361575
3502.955613	701918.235986	42.366580
3502.567250	701868.807066	42.371584
3502.769407	701808.397973	42.376589
3502.787859	701751.994135	42.381594
3502.712774	701705.046986	42.386599
3503.090908	701645.154387	42.391604
3502.473632	701587.562212	42.396608
3502.575750	701522.943676	42.401613
3502.771546	701495.033182	42.406618
3502.575193	701436.525854	42.411623
3502.878561	701372.668154	42.416628
3502.510043	701329.096873	42.421632
3502.366647	701283.102911	42.426637
3502.393528	701222.420467	42.431642
3502.493741	701176.037930	42.436647
3502.482190	701132.108672	42.441652
3502.232092	701082.205239	42.446656
3502.689210	701017.922039	42.451661
3502.591671	700981.808577	42.456666
3502.338818	700929.221087	42.461671
3502.463673	700878.161366	42.466676
3502.431185	700837.215924	42.471680
3502.418389	700781.457030	42.476685
3502.479725	700738.458044	42.481690
3502.381550	700694.491158	42.486695
3502.559890	700651.223971	42.491700
3502.464705	700594.234986	42.496704
3502.663764	700547.335832	42.501709
3502.575262	700485.772691	42.506714
3502.340036	700437.503213	42.511719
3502.543759	700375.046241	42.516724
3502.315286	700341.039118	42.521728
3502.467563	700282.069000	42.526733
3502.360363	700235.119233	42.531738
3502.056410	700178.311038	42.536743
3502.209029	700136.785097	42.541748
3501.931314	700099.007812	42.546752
3502.469629	700051.801592	42.551757
3502.049001	700008.480812	42.556762
3501.952764	699968.436448	42.561767
3502.250541	699926.438267	42.566772
3502.291363	699887.414711	42.571776
3502.428911	699848.474450	42.576781
3502.802833	699794.633678	42.581786
3502.225679	699750.393039	42.586791
3502.494735	699703.577239	42.591796
3502.364331	699655.534692	42.596800
3502.479466	699601.238328	42.601805
3502.608516	699544.802014	42.606810
3502.211403	699489.694670	42.611815
3502.639239	699455.078906	42.616820
3502.057120	699409.545014	42.621824
3502.622814	699360.044091	42.626829
3502.287843	699298.960566	42.631834
3502.128333	699261.706959	42.636839
3502.409358	699221.249069	42.641844
3502.404859	699167.615921	42.646848
3502.271141	699107.939413	42.651853
3502.514952	699071.612694	42.656858
3502.338759	699038.735173	42.661863
3502.525998	698970.554486	42.666868
3502.414035	698940.946766	42.671872
3502.283715	698885.592826	42.676877
3502.367248	698838.355599	42.681882
3502.331282	698787.658150	42.686887
3502.268964	698739.002847	42.691892
3501.761172	698707.570593	42.696896
3502.263395	698663.444866	42.701901
3502.370851	698622.416296	42.706906
3502.136415	698583.730554	42.711911
3502.172239	698533.666047	42.716916
3501.877258	698489.720516	42.721920
3502.075471	698458.469305	42.726925
3502.301759	698410.808566	42.731930
3501.978448	698353.942015	42.736935
3502.196055	698316.821104	42.741940
3501.827842	698274.427635	42.746944
3502.324957	698237.061484	42.751949
3502.327108	698197.191667	42.756954
3502.206364	698151.823779	42.761959
3502.392225	698101.732089	42.766964
3502.202221	698063.981288	42.771968
3502.286555	698009.978438	42.776973
3502.188179	697964.357327	42.781978
3501.958783	697927.507283	42.786983
3502.356037	697877.826916	42.791988
3501.928980	697840.661075	42.796993
3502.161374	697798.116630	42.801997
3502.187915	697755.257891	42.807002
3502.294591	697713.777773	42.812007
3502.054492	697661.466851	42.817012
3502.130004	697621.482906	42.822017
3502.239380	697579.504551	42.827021
3502.137188	697549.791099	42.832026
3502.103121	697494.909702	42.837031
3501.816491	697449.416373	42.842036
3502.017735	697414.879638	42.847041
3501.614825	697373.133861	42.852045
3501.989690	697351.494784	42.857050
3502.178808	697309.203696	42.862055
3502.193199	697266.792042	42.867060
3502.006180	697226.153508	42.872065
3501.831521	697176.911453	42.877069
3501.894356	697145.031548	42.882074
3501.664560	697095.400373	42.887079
3501.932158	697055.034174	42.892084
3501.968503	697033.897570	42.897089
3501.686422	696988.699427	42.902093
3502.026277	696949.563829	42.907098
3502.132151	696902.113647	42.912103
3501.897325	696858.796412	42.917108
3501.496199	696817.942673	42.922113
3501.889526	696801.967347	42.927117
3502.032703	696753.515806	42.932122
3501.849396	696717.050867	42.937127
3502.110631	696665.098911	42.942132
3502.084793	696622.243293	42.947137
3501.965980	696593.871840	42.952141
3502.200547	696553.260182	42.957146
3502.005189	696524.602786	42.962151
3502.204968	696474.648723	42.967156
3501.928528	696439.192430	42.972161
3502.342971	696397.754856	42.977165
3502.207335	696356.009941	42.982170
3502.253154	696318.560861	42.987175
3502.168156	696269.000622	42.992180
3502.008561	696222.734174	42.997185
3501.966449	696183.310054	43.002189
3502.224052	696145.676173	43.007194
3502.035796	696102.993970	43.012199
3502.233986	696058.059993	43.017204
3502.174660	696023.162952	43.022209
3502.319915	695963.071075	43.027213
3502.189032	695922.616187	43.032218
3502.040257	695872.368074	43.037223
3502.132960	695828.544282	43.042228
3501.893890	695791.985257	43.047233
3502.262222	695750.850610	43.052237
3502.004628	695713.946228	43.057242
3501.815188	695670.118414	43.062247
3501.893267	695626.246302	43.067252
3501.628051	695595.011583	43.072257
3501.443979	695560.033812	43.077261
3501.764345	695536.708541	43.082266
3501.824187	695488.462709	43.087271
3502.104273	695447.788748	43.092276
3502.088023	695404.776461	43.097281
3502.266867	695367.599807	43.102285
3502.034465	695323.876813	43.107290
3501.879911	695291.528751	43.112295
3502.060735	695248.085398	43.117300
3501.771316	695198.005816	43.122305
3501.882348	695176.703276	43.127309
3501.864643	695129.363402	43.132314
3501.669068	695085.036399	43.137319
3501.750978	695048.421411	43.142324
3501.721793	695029.578415	43.147329
3501.406699	694990.641535	43.152333
3501.950948	694958.923076	43.157338
3501.770859	694929.014714	43.162343
3501.756350	694883.363857	43.167348
3501.884933	694860.615455	43.172353
3501.965330	694813.556118	43.177357
3501.897743	694775.174290	43.182362
3501.691964	694737.163191	43.187367
3501.800095	694698.702346	43.192372
3501.446128	694673.596086	43.197377
3501.653128	694636.212795	43.202381
3501.658582	694602.443333	43.207386
3501.541389	694560.189574	43.212391
3501.952194	694529.486235	43.217396
3501.693000	694495.660506	43.222401
3501.910148	694455.638904	43.227405
3501.945574	694425.444663	43.232410
3501.522766	694393.933267	43.237415
3501.722546	694353.118318	43.242420
3501.616124	694326.876129	43.247425
3501.735335	694288.610619	43.252429
3501.650056	694245.355408	43.257434
3501.565987	694211.698679	43.262439
3501.651521	694183.633971	43.267444
3501.942966	694149.915134	43.272449
3501.583132	694100.388042	43.277453
3501.921198	694070.490878	43.282458
3501.771545	694036.595612	43.287463
3502.115421	694000.181816	43.292468
3501.720970	693968.813445	43.297473
3501.566979	693925.816681	43.302477
3501.803998	693901.406642	43.307482
3501.696491	693864.071926	43.312487
3501.850333	693826.892939	43.317492
3501.705493	693786.032696	43.322497
3501.753560	693753.993800	43.327501
3501.918047	693721.587440	43.332506
3501.620263	693684.183845	43.337511
3501.601849	693649.022022	43.342516
3501.599221	693608.883607	43.347521
3501.571466	693577.751863	43.352525
3501.917818	693547.055756	43.357530
3501.522470	693530.110249	43.362535
3501.939165	693477.417653	43.367540
3501.484145	693451.280055	43.372545
3501.995911	693402.152587	43.377549
3502.087928	693373.736077	43.382554
3501.799783	693339.363573	43.387559
3502.038969	693296.647161	43.392564
3501.863519	693275.387268	43.397569
3501.878066	693229.474421	43.402573
3501.913764	693194.948517	43.407578
3501.748743	693155.929115	43.412583
3502.075924	693117.375594	43.417588
3501.761054	693083.653142	43.422593
3501.762148	693044.406913	43.427597
3501.917626	693008.666750	43.432602
3501.725174	692973.978614	43.437607
3501.841727	692942.024995	43.442612
3501.920388	692902.168452	43.447617
3501.692949	692867.585152	43.452621
3502.180211	692821.293855	43.457626
3501.984323	692788.545537	43.462631
3502.114784	692735.845979	43.467636
3501.926518	692707.224810	43.472641
3501.937134	692663.349180	43.477645
3502.046379	692619.606315	43.482650
3501.988595	692585.640638	43.487655
3501.550744	692542.634217	43.492660
3501.842902	692511.097820	43.497665
3501.646712	692477.502749	43.502669
3501.594630	692450.897856	43.507674
3501.741383	692409.436050	43.512679
3501.870106	692364.594330	43.517684
3501.762802	692339.689551	43.522689
3501.599835	692302.456914	43.527693
3501.854830	692252.768479	43.532698
3501.721834	692224.335636	43.537703
3501.792943	692190.695440	43.542708
3501.662846	692159.177631	43.547713
3501.612444	692123.169364	43.552717
3501.703983	692079.476516	43.557722
3501.385408	692049.083809	43.562727
3501.922075	692019.047552	43.567732
3501.316832	691985.717018	43.572737
3501.458024	691963.456614	43.577741
3501.669032	691939.592719	43.582746
3501.360986	691911.535957	43.587751
3501.596763	691869.410252	43.592756
3501.842441	691837.431403	43.597761
3501.758418	691787.050012	43.602765
3502.065512	691762.274335	43.607770
3501.799418	691724.210547	43.612775
3501.778055	691693.518911	43.617780
3501.831632	691656.397146	43.622785
3501.928281	691610.512188	43.627789
3501.986657	691587.020750	43.632794
3501.533588	691533.763499	43.637799
3501.584834	691500.173728	43.642804
3501.745226	691472.336901	43.647809
3501.616349	691434.398520	43.652813
3501.652684	691400.213822	43.657818
3501.669562	691367.425229	43.662823
3501.945185	691327.628706	43.667828
3502.147711	691299.635147	43.672833
3501.858444	691270.229986	43.677837
3501.859721	691219.930847	43.682842
3501.638500	691181.807603	43.687847
3501.809874	691144.515048	43.692852
3501.653269	691108.420687	43.697857
3501.645415	691074.242025	43.702861
3502.052466	691042.034734	43.707866
3501.519515	691007.594069	43.712871
3501.489014	690966.254284	43.717876
3501.568761	690934.548318	43.722881
3501.446319	690904.169149	43.727885
3501.950185	690878.761564	43.732890
3501.538900	690852.658883	43.737895
3502.026417	690796.505791	43.742900
3501.634857	690769.255268	43.747905
3501.688946	690733.970505	43.752909
3501.844121	690701.952760	43.757914
3501.610573	690670.098461	43.762919
3501.518633	690628.120426	43.767924
3501.889585	690598.355493	43.772929
3501.595186	690556.808526	43.777933
3501.742367	690519.268578	43.782938
3501.384023	690487.085901	43.787943
3501.955605	690466.193781	43.792948
3501.546962	690430.536264	43.797953
3501.832073	690395.958448	43.802957
3501.338153	690360.513730	43.807962
3501.403038	690333.037398	43.812967
3501.469788	690293.917543	43.817972
3501.371526	690266.418133	43.822977
3501.318093	690237.617561	43.827981
3501.713028	690208.743019	43.832986
3501.357252	690183.773660	43.837991
3501.585745	690142.884978	43.842996
3501.689553	690116.197695	43.848001
3501.536912	690084.875322	43.853005
3501.886580	690061.232371	43.858010
3501.315889	690041.522648	43.863015
3501.504398	690009.944767	43.868020
3501.519858	689967.547873	43.873025
3501.442048	689938.451805	43.878029
3502.050447	689897.698446	43.883034
3501.559268	689875.736091	43.888039
3501.767128	689841.616705	43.893044
3501.543318	689812.643805	43.898049
3501.368445	689766.346307	43.903053
3501.494725	689727.164414	43.908058
3501.592570	689703.960099	43.913063
3501.806688	689668.196933	43.918068
3501.511318	689642.818030	43.923073
3501.566466	689599.069320	43.928077
3501.564554	689575.483024	43.933082
3501.450783	689541.763823	43.938087
3501.726322	689495.888327	43.943092
3501.531080	689482.086876	43.948097
3501.250342	689449.887687	43.953101
3501.768829	689418.651452	43.958106
3501.499388	689392.521140	43.963111
3501.380697	689354.174177	43.968116
3501.545959	689317.322898	43.973121
3501.048871	689283.417075	43.978125
3501.556337	689266.264935	43.983130
3501.367573	689235.791518	43.988135
3501.588270	689201.816878	43.993140
3501.297834	689172.554312	43.998145
3501.584823	689141.006917	44.003149
3501.799836	689107.480728	44.008154
3501.480090	689087.030863	44.013159
3501.554526	689046.063051	44.018164
3501.494458	689013.925466	44.023169
3501.412685	688981.691814	44.028173
3501.682082	688945.120439	44.033178
3501.275300	688916.771971	44.038183
3501.501783	688885.134121	44.043188
3501.358851	688862.614252	44.048193
3501.026383	688838.582841	44.053197
3501.582657	688804.302582	44.058202
3501.377197	688768.754275	44.063207
3501.291271	688737.913867	44.068212
3501.115717	688714.204627	44.073217
3501.124263	688692.405859	44.078221
3501.380803	688659.966012	44.083226
3500.938944	688651.130757	44.088231
3501.115482	688614.175211	44.093236
3501.144371	688602.375896	44.098241
3501.293935	688576.572301	44.103245
3501.429033	688546.889216	44.108250
3501.175340	688516.822194	44.113255
3501.115992	688493.391825	44.118260
3501.399729	688461.543987	44.123265
3501.514801	688453.711648	44.128269
3501.385109	688416.357845	44.133274
3501.080887	688401.129435	44.138279
3501.269908	688360.935907	44.143284
3501.299703	688332.414124	44.148289
3500.977055	688298.077696	44.153293
3501.216628	688283.506005	44.158298
3501.293991	688261.943697	44.163303
3501.103766	688228.132633	44.168308
3501.307425	688195.152376	44.173313
3501.048013	688191.711383	44.178317
3501.526317	688146.243525	44.183322
3501.142358	688134.262779	44.188327
3501.396849	688089.578047	44.193332
3501.441137	688076.979200	44.198337
3501.294073	688037.536380	44.203341
3501.645307	688017.720063	44.208346
3501.283367	687992.297698	44.213351
3501.051282	687954.311845	44.218356
3501.022018	687936.897235	44.223361
3501.206680	687918.004008	44.228365
3501.464757	687881.927890	44.233370
3501.391692	687855.113738	44.238375
3501.406198	687836.696313	44.243380
3501.255128	687806.261615	44.248385
3501.071885	687783.098669	44.253389
3501.473720	687735.600738	44.258394
3501.003023	687731.597128	44.263399
3501.436998	687695.491283	44.268404
3501.236081	687675.267483	44.273409
3501.208300	687637.644804	44.278413
3501.440324	687614.263685	44.283418
3501.145493	687586.440068	44.288423
3501.339997	687566.349957	44.293428
3501.237788	687532.422237	44.298433
3501.102176	687518.408858	44.303437
3501.315246	687489.456033	44.308442
3501.090736	687469.384977	44.313447
3501.156664	687430.203042	44.318452
3501.381250	687399.804621	44.323457
3501.034247	687373.631453	44.328461
3501.199646	687358.124804	44.333466
3501.148667	687328.219507	44.338471
3501.328231	687300.067972	44.343476
3501.247002	687285.298666	44.348481
3500.966156	687261.105216	44.353485
3501.461637	687223.245271	44.358490
3501.158541	687207.616464	44.363495
3501.118768	687171.835462	44.368500
3501.243880	687143.891510	44.373505
3501.000640	687124.768487	44.378509
3501.304004	687088.980392	44.383514
3501.067392	687085.286342	44.388519
3501.195534	687045.893392	44.393524
3501.299850	687030.844222	44.398529
3501.122487	686992.895081	44.403533
3501.314877	686979.274795	44.408538
3500.812811	686964.673858	44.413543
3501.099476	686931.326886	44.418548
3501.248026	686896.608827	44.423553
3501.101369	686874.184157	44.428557
3501.591819	686848.518563	44.433562
3501.431463	686828.236406	44.438567
3501.334527	686799.382232	44.443572
3501.492787	686782.282932	44.448577
3501.290229	686756.382832	44.453581
3501.425900	686719.625378	44.458586
3501.311433	686695.452774	44.463591
3501.705795	686661.887958	44.468596
3501.507021	686639.073076	44.473601
3501.344572	686599.427402	44.478605
3501.627660	686577.379182	44.483610
3501.428361	686558.297497	44.488615
3501.467442	686510.156023	44.493620
3501.279351	686488.135446	44.498625
3501.254692	686461.458518	44.503629
3501.589640	686427.454621	44.508634
3501.578447	686393.109403	44.513639
3501.438400	686369.487707	44.518644
3501.523354	686341.647456	44.523649
3501.332870	686318.681063	44.528653
3501.326338	686273.681922	44.533658
3501.108840	686258.336042	44.538663
3501.289610	686234.561574	44.543668
3501.543222	686197.085656	44.548673
3501.193866	686178.724810	44.553677
3501.536501	686143.523869	44.558682
3501.277418	686128.483300	44.563687
3501.508850	686100.120371	44.568692
3501.214911	686065.720941	44.573697
3500.995660	686042.907929	44.578701
3501.443258	686008.037631	44.583706
3501.049609	685978.084775	44.588711
3501.342486	685948.715633	44.593716
3501.182416	685937.143099	44.598721
3501.193922	685913.146774	44.603725
3501.211304	685884.818442	44.608730
3501.257435	685861.264307	44.613735
3501.322268	685837.458121	44.618740
3501.389301	685815.543215	44.623745
3501.063637	685774.676282	44.628749
3501.289528	685748.503574	44.633754
3501.342719	685738.090415	44.638759
3501.107703	685704.874677	44.643764
3501.201197	685660.503183	44.648769
3501.172006	685651.796107	44.653773
3501.573993	685634.106876	44.658778
3501.199812	685595.885614	44.663783
3501.536441	685559.986442	44.668788
3501.413678	685531.729884	44.673793
3501.295388	685513.678097	44.678797
3501.387975	685475.578551	44.683802
3501.308917	685449.355662	44.688807
3501.059446	685427.591539	44.693812
3501.273742	685403.311533	44.698817
3500.986262	685369.904077	44.703821
3501.236135	685352.786990	44.708826
3501.140157	685325.421492	44.713831
3501.165068	685291.563999	44.718836
3501.546708	685278.905673	44.723841
3501.367520	685247.969157	44.728845
3501.599730	685208.302155	44.733850
3501.250491	685200.543513	44.738855
3501.270542	685155.434877	44.743860
3501.114222	685132.957703	44.748865
3501.106865	685107.170080	44.753869
3501.207961	685094.059869	44.758874
3501.119677	685072.019405	44.763879
3501.572975	685047.450139	44.768884
3501.142408	685010.082061	44.773889
3500.974252	684990.842584	44.778893
3501.384830	684956.870511	44.783898
3500.976700	684939.064485	44.788903
3500.947461	684908.550184	44.793908
3501.151077	684892.286227	44.798913
3501.407110	684884.776088	44.803917
3501.152460	684853.551942	44.808922
3501.230512	684808.083517	44.813927
3501.185838	684788.873053	44.818932
3501.611920	684760.473873	44.823937
3501.428510	684749.650482	44.828941
3501.708335	684703.152535	44.833946
3501.275342	684673.052487	44.838951
3501.324647	684642.076258	44.843956
3501.210061	684616.454277	44.848961
3501.240619	684594.940746	44.853965
3501.336824	684551.360007	44.858970
3501.250790	684536.686590	44.863975
3501.387703	684507.189129	44.868980
3501.330997	684483.349635	44.873985
3501.110157	684463.271309	44.878989
3501.196944	684433.632501	44.883994
3500.927179	684406.043926	44.888999
3501.028914	684380.535004	44.894004
3500.923851	684369.548881	44.899009
3501.279316	684336.131262	44.904013
3501.723388	684318.681496	44.909018
3501.188480	684292.779332	44.914023
3501.338780	684261.287267	44.919028
3501.333269	684233.355884	44.924033
3501.045264	684203.031227	44.929037
3501.269726	684170.530817	44.934042
3501.180748	684165.217937	44.939047
3501.175367	684131.211746	44.944052
3501.561109	684108.742305	44.949057
3501.255619	684087.930232	44.954061
3501.344481	684055.800296	44.959066
3500.903472	684026.745045	44.964071
3501.164966	684006.387068	44.969076
3501.134495	683977.413390	44.974081
3501.195085	683950.565667	44.979085
3501.350907	683913.644171	44.984090
3501.232729	683905.547591	44.989095
3501.075049	683882.519838	44.994100
3501.604040	683854.947354	44.999105
3501.479379	683819.117332	45.004109
3501.617585	683780.804007	45.009114
3501.494512	683763.795184	45.014119
3501.418425	683726.214041	45.019124
3501.302766	683687.195256	45.024129
3501.352156	683678.622723	45.029133
3501.438613	683637.728067	45.034138
3501.213360	683611.275001	45.039143
3501.414013	683590.029834	45.044148
3501.297053	683560.820114	45.049153
3501.050222	683530.486432	45.054157
3501.510720	683500.882605	45.059162
3501.441609	683493.225723	45.064167
3501.558157	683465.520849	45.069172
3501.689232	683429.846338	45.074177
3501.178934	683392.783520	45.079181
3501.902598	683357.957190	45.084186
3501.573227	683327.935207	45.089191
3501.233145	683300.753231	45.094196
3501.437597	683277.016937	45.099201
3501.357623	683249.244197	45.104205
3501.264944	683218.186936	45.109210
3501.144342	683198.089303	45.114215
3501.032866	683165.142710	45.119220
3501.074982	683140.486682	45.124225
3501.072639	683117.879569	45.129229
3501.391388	683100.248946	45.134234
3501.391233	683074.653572	45.139239
3501.451250	683043.122385	45.144244
3501.390263	683012.706563	45.149249
3501.227222	682980.166176	45.154253
3501.573795	682954.015360	45.159258
3501.516978	682927.731747	45.164263
3501.471589	682902.093545	45.169268
3501.317294	682868.057388	45.174273
3501.104592	682849.368502	45.179277
3501.328151	682806.804205	45.184282
3501.140706	682791.646707	45.189287
3501.142638	682768.440447	45.194292
3501.231197	682737.750077	45.199297
3501.260901	682708.712658	45.204301
3501.403910	682685.980930	45.209306
3501.472299	682662.663853	45.214311
3501.349009	682628.024106	45.219316
3501.176905	682593.541668	45.224321
3500.936008	682570.872912	45.229325
3501.166199	682547.977077	45.234330
3501.346934	682525.886129	45.239335
3501.279104	682490.489727	45.244340
3501.360831	682476.681751	45.249345
3501.182141	682447.279442	45.254349
3501.301984	682412.947419	45.259354
3501.101842	682389.922896	45.264359
3500.958392	682366.888973	45.269364
3501.679895	682328.473451	45.274369
3501.137267	682319.499187	45.279373
3501.282733	682291.736192	45.284378
3500.972575	682271.468551	45.289383
3501.162496	682241.008819	45.294388
3501.096167	682212.483663	45.299393
3501.097229	682185.042947	45.304397
3501.075846	682161.241371	45.309402
3501.016868	682136.599296	45.314407
3500.847846	682104.305786	45.319412
3501.188346	682094.538357	45.324417
3501.225053	682074.810750	45.329421
3501.007997	682051.290140	45.334426
3500.983818	682022.906855	45.339431
3501.135619	682009.385443	45.344436
3501.263351	681977.142192	45.349441
3500.803093	681949.826588	45.354445
3501.179020	681936.019124	45.359450
3501.139892	681911.671991	45.364455
3501.013405	681885.795290	45.369460
3501.211556	681858.868958	45.374465
3501.057212	681838.624486	45.379469
3501.126078	681817.197709	45.384474
3501.115079	681802.806354	45.389479
3500.951686	681780.272278	45.394484
3500.957640	681744.113778	45.399489
3500.614912	681739.887178	45.404493
3501.275460	681704.019092	45.409498
3501.038022	681688.519373	45.414503
3501.379263	681669.139148	45.419508
3501.454596	681653.587834	45.424513
3501.254005	681615.570292	45.429517
3501.272650	681591.860251	45.434522
3501.206150	681568.164178	45.439527
3500.976436	681549.126803	45.444532
3500.993732	681512.766302	45.449537
3500.815931	681498.999617	45.454541
3501.028881	681467.935862	45.459546
3501.121249	681438.983705	45.464551
3501.051704	681421.862092	45.469556
3500.952222	681397.523539	45.474561
3500.927794	681386.171898	45.479565
3500.543268	681359.389917	45.484570
3500.941710	681342.489879	45.489575
3500.730481	681328.429610	45.494580
3501.248194	681309.119161	45.499585
3501.234015	681297.915141	45.504589
3501.185070	681261.664173	45.509594
3501.360844	681238.923461	45.514599
3501.122325	681213.959843	45.519604
3501.188440	681183.965266	45.524609
3500.931838	681174.643898	45.529613
3501.146783	681135.659371	45.534618
3501.295745	681118.600802	45.539623
3500.925742	681088.428737	45.544628
3501.099042	681059.312626	45.549633
3500.995060	681045.383674	45.554637
3501.144417	681027.727178	45.559642
3501.282368	681013.310043	45.564647
3501.243746	680990.155771	45.569652
3501.454857	680964.818540	45.574657
3501.451307	680930.650728	45.579661
3501.543332	680890.788867	45.584666
3501.376955	680865.264519	45.589671
3501.169948	680841.539914	45.594676
3501.484862	680825.798296	45.599681
3501.200654	680793.319913	45.604685
3501.232985	680761.934870	45.609690
3501.485311	680738.482977	45.614695
3501.153023	680709.947163	45.619700
3501.630615	680685.461826	45.624705
3501.423718	680651.774771	45.629709
3501.304281	680617.176601	45.634714
3501.380461	680575.522821	45.639719
3501.345293	680561.830848	45.644724
3501.361948	680534.930545	45.649729
3501.139733	680513.349448	45.654733
3501.318810	680470.582406	45.659738
3501.585242	680443.391623	45.664743
3501.104672	680421.055904	45.669748
3500.987228	680404.338776	45.674753
3501.133129	680367.753309	45.679757
3500.933474	680344.972626	45.684762
3500.998995	680324.041034	45.689767
3501.112505	680309.427578	45.694772
3501.205116	680273.249010	45.699777
3500.737518	680263.264115	45.704781
3500.813499	680247.710317	45.709786
3500.933748	680211.128454	45.714791
3501.036122	680194.773222	45.719796
3501.286180	680180.635185	45.724801
3501.359235	680166.576105	45.729805
3501.154356	680137.668831	45.734810
3501.230366	680103.783715	45.739815
3501.355611	680067.798215	45.744820
3501.304031	680034.232744	45.749825
3501.129980	679947.187602	45.754829
3501.042889	679808.718968	45.759834
3500.831071	679630.964554	45.764839
3500.795848	679368.190542	45.769844
3500.535044	679066.438470	45.774849
3500.390849	678723.854606	45.779853
3500.182799	678301.353535	45.784858
3499.818386	677835.909838	45.789863
3499.469842	677309.849628	45.794868
3499.281975	676719.949585	45.799873
3498.479647	676082.372042	45.804877
3498.421945	675376.898192	45.809882
3497.984405	674634.002138	45.814887
3497.578726	673814.427888	45.819892
3497.025275	672937.926158	45.824897
3495.968535	672014.161993	45.829901
3495.485860	671027.836159	45.834906
3494.901093	669987.218901	45.839911
3493.859713	668887.413627	45.844916
3493.225479	667737.934228	45.849921
3492.629462	666523.708785	45.854925
3491.943566	665258.903421	45.859930
3490.982911	663924.867078	45.864935
3490.028768	662549.971493	45.869940
3489.312811	661107.757748	45.874945
3488.051430	659605.464421	45.879949
3486.864762	658052.698501	45.884954
3485.837244	656446.576644	45.889959
3484.379339	654789.618276	45.894964
3483.667300	653068.317382	45.899969
3482.154542	651304.530716	45.904973
3480.633170	649481.365989	45.909978
3479.460088	647608.529955	45.914983
3478.245877	645695.209228	45.919988
3476.919491	643714.544149	45.924993
3475.279387	641690.485791	45.929997
3473.881488	639621.418432	45.935002
3471.961489	637509.994915	45.940007
3470.313472	635347.954322	45.945012
3468.744988	633122.936808	45.950017
3467.239596	630872.254848	45.955021
3465.535895	628571.502389	45.960026
3463.599002	626226.215356	45.965031
3461.988363	623836.526261	45.970036
3460.161344	621400.995539	45.975041
3457.855501	618915.128830	45.980045
3456.124778	616402.433762	45.985050
3453.702913	613845.806250	45.990055
3451.421650	611252.205119	45.995060
3449.967302	608622.650139	46.000065
3447.578971	605955.504683	46.005069
3445.760749	603243.272319	46.010074
3443.314863	600492.549605	46.015079
3440.838029	597715.418031	46.020084
3438.864758	594880.084603	46.025089
3436.362439	592035.765265	46.030093
3434.116805	589143.387262	46.035098
3431.709066	586224.905333	46.040103
3429.140776	583266.884005	46.045108
3427.038849	580276.288488	46.050113
3424.298353	577248.908505	46.055117
3421.774619	574192.180531	46.060122
3419.402037	571101.723624	46.065127
3416.483002	567992.937925	46.070132
3413.798908	564845.852590	46.075137
3410.810279	561682.342671	46.080141
3408.192926	558476.906098	46.085146
3405.646527	555253.855790	46.090151
3402.582661	552005.221657	46.095156
3400.084355	548735.100590	46.100161
3397.053363	545433.129839	46.105165
3394.112117	542111.852021	46.110170
3390.991262	538761.471033	46.115175
3387.897185	535392.588394	46.120180
3384.815421	532002.326993	46.125185
3382.185715	528588.237224	46.130189
3378.979996	525162.751822	46.135194
3376.133365	521712.386786	46.140199
3372.827897	518237.220264	46.145204
3370.038555	514735.367855	46.150209
3366.403890	511210.180525	46.155213
3363.413347	507682.234157	46.160218
3360.343681	504127.945720	46.165223
3356.557025	500571.587041	46.170228
3353.898096	496992.581681	46.175233
3349.822352	493385.579182	46.180237
3346.774279	489771.474189	46.185242
3343.519236	486141.823419	46.190247
3339.786360	482506.292511	46.195252
3336.737476	478848.800095	46.200257
3333.171606	475199.777246	46.205261
3329.525956	471517.026464	46.210266
3326.235752	467829.093275	46.215271
3322.781662	464142.255180	46.220276
3319.252909	460419.158688	46.225281
3315.456181	456704.284339	46.230285
3312.432413	452970.353670	46.235290
3308.342960	449225.228386	46.240295
3305.069285	445481.538726	46.245300
3301.512641	441715.029728	46.250305
3297.973466	437967.966797	46.255309
3293.890623	434193.832267	46.260314
3290.570097	430411.696677	46.265319
3286.843066	426619.275304	46.270324
3283.192534	422836.398321	46.275329
3279.384534	419047.305839	46.280333
3275.747856	415227.400926	46.285338
3272.320184	411427.112497	46.290343
3268.018354	407620.963268	46.295348
3264.264171	403809.060361	46.300353
3260.554979	399998.535546	46.305357
3256.800229	396181.897067	46.310362
3252.938540	392365.316300	46.315367
3249.067631	388549.655147	46.320372
3245.453317	384716.480980	46.325377
3241.414881	380892.326635	46.330381
3237.643535	377073.357830	46.335386
3233.945677	373241.085708	46.340391
3229.812029	369421.084523	46.345396
3225.743459	365590.451071	46.350401
3221.663255	361777.288850	46.355405
3218.072207	357954.468830	46.360410
3214.301686	354142.616719	46.365415
3210.226939	350330.778858	46.370420
3206.497019	346511.610345	46.375425
3202.363873	342710.081822	46.380429
3198.510545	338900.192327	46.385434
3194.916789	335093.689322	46.390439
3190.678645	331285.798541	46.395444
3186.994694	327473.586676	46.400449
3183.075351	323671.986038	46.405453
3178.871225	319865.822728	46.410458
3174.678312	316070.208124	46.415463
3170.727363	312285.399405	46.420468
3167.089525	308498.644138	46.425473
3162.952546	304723.303851	46.430477
3158.688521	300953.577345	46.435482
3154.792722	297183.030876	46.440487
3150.691314	293434.078961	46.445492
3146.675598	289676.894354	46.450497
3142.626113	285935.064952	46.455501
3138.926592	282186.131015	46.460506
3135.013464	278461.649634	46.465511
3130.479440	274736.667574	46.470516
3126.810481	271007.947231	46.475521
3122.538555	267295.379052	46.480525
3118.468702	263592.221548	46.485530
3114.582455	259907.709876	46.490535
3110.464520	256215.234173	46.495540
3106.559979	252529.937861	46.500545
3102.430571	248862.168972	46.505549
3098.449324	245192.191130	46.510554
3094.388541	241533.857367	46.515559
3090.255301	237891.914879	46.520564
3086.444025	234254.645978	46.525569
3082.248905	230632.263034	46.530573
3078.147274	227005.064253	46.535578
3074.376877	223392.681060	46.540583
3069.975681	219796.224488	46.545588
3066.246486	216198.811446	46.550593
3062.159936	212610.069491	46.555597
3058.261832	209040.956160	46.560602
3054.235376	205379.039296	46.565607
3050.170156	201821.070677	46.570612
3046.167066	198271.425862	46.575617
3041.730514	194725.194251	46.580621
3037.994847	191203.135293	46.585626
3034.090576	187680.188070	46.590631
3029.492831	184175.258450	46.595636
3025.039190	180665.718194	46.600641
3021.093581	177183.112209	46.605645
3017.315068	173713.175545	46.610650
3013.364174	170250.882974	46.615655
3009.050930	166812.710034	46.620660
3005.292198	163366.048386	46.625665
3001.058389	159943.602553	46.630669
2997.307586	156525.022370	46.635674
2993.095911	153116.818120	46.640679
2989.025517	149725.242775	46.645684
2984.991090	146355.239472	46.650689
2980.711649	142981.253323	46.655693
2976.698219	139607.367583	46.660698
2972.921776	136258.662446	46.665703
2968.446398	132929.740012	46.670708
2964.788646	129596.677757	46.675713
2960.157907	126294.293586	46.680717
2956.050813	123007.296507	46.685722
2952.380731	119717.347094	46.690727
2947.774918	116456.374981	46.695732
2943.875695	113196.952831	46.700737
2939.881892	109965.738082	46.705741
2935.413392	106737.408092	46.710746
2931.511276	103513.969713	46.715751
2927.054869	100333.128690	46.720756
2922.958839	97136.310549	46.725761
2918.739915	93979.923581	46.730765
2914.209103	90836.428030	46.735770
2909.952136	87724.020950	46.740775
2905.492923	84611.458362	46.745780
2901.790900	81518.772082	46.750785
2896.929739	78466.742752	46.755789
2892.667431	75399.911230	46.760794
2888.084538	72380.194887	46.765799
2883.458384	69388.353112	46.770804
2878.888416	66407.397045	46.775809
2874.158101	63469.450939	46.780813
2869.336528	60558.213198	46.785818
2864.205881	57676.287005	46.790823
2858.554340	54843.059905	46.795828
2852.437972	52058.444484	46.800833
2843.894478	49400.005279	46.805837
2834.407202	46840.798916	46.810842
2825.084232	44362.927128	46.815847
2816.096378	42004.177537	46.820852
2807.579935	39745.303804	46.825857
2798.971367	37598.877801	46.830861
2791.348836	35574.566410	46.835866
2783.770393	33648.371788	46.840871
2776.671529	31826.310650	46.845876
2769.792623	30096.321666	46.850881
2762.608555	28479.416793	46.855885
2756.194200	26937.345567	46.860890
2750.294653	25476.879574	46.865895
2744.544233	24119.327544	46.870900
2738.484301	22818.047195	46.875905
2732.753234	21595.956547	46.880909
2726.906818	20436.026482	46.885914
2721.527862	19355.207929	46.890919
2715.586852	18346.730080	46.895924
2710.182007	17398.076453	46.900929
2704.318421	16517.152776	46.905933
2699.014899	15686.702553	46.910938
2694.031566	14916.709905	46.915943
2688.608716	14206.419633	46.920948
2683.951949	13529.274692	46.925953
2678.762499	12911.360820	46.930957
2674.190082	12338.837361	46.935962
2669.840916	11788.069492	46.940967
2665.373096	11282.287580	46.945972
2661.371650	10801.348187	46.950977
2657.244625	10350.395656	46.955981
2653.380309	9919.252574	46.960986
2649.882061	9503.601276	46.965991
2646.214218	9131.074389	46.970996
2642.882399	8754.318737	46.976001
2639.419294	8395.080771	46.981005
2635.729009	8027.547729	46.986010
2632.788624	7692.855197	46.991015
2629.298117	7356.881600	46.996020
2626.338756	7025.001030	47.001025
2623.152105	6691.151959	47.006029
2619.746672	6371.979450	47.011034
2616.554418	6046.808357	47.016039
2613.137787	5730.207515	47.021044
2610.350207	5401.615836	47.026049
2607.305255	5077.653189	47.031053
2603.970800	4767.130950	47.036058
2600.919417	4441.655333	47.041063
2597.505044	4120.817116	47.046068
2594.378491	3802.308949	47.051073
2591.049463	3472.599713	47.056077
2587.869039	3154.172002	47.061082
2584.482527	2835.870035	47.066087
2580.671076	2515.280960	47.071092
2577.740120	2189.909517	47.076097
2574.089182	1875.802009	47.081101
2570.748560	1568.484536	47.086106
2567.039678	1247.549342	47.091111
2562.855847	937.763804	47.096116
2558.921614	639.624207	47.101121
2555.029910	362.217371	47.106125
2548.667938	147.666522	47.111130
2534.681898	191.309815	47.116135
2524.730227	190.678555	47.121140
2519.713930	187.599174	47.126145
2517.270201	182.488859	47.131149
2515.670445	181.941886	47.136154
2514.502125	183.943999	47.141159
2512.166816	179.504513	47.146164
2509.861929	178.046169	47.151169
2506.747623	169.896587	47.156173
2503.312233	175.449069	47.161178
2500.577116	170.739113	47.166183
2496.680126	182.177498	47.171188
2493.304554	170.384918	47.176193
2490.374066	171.726696	47.181197
2486.508392	187.652185	47.186202
2483.456868	167.612937	47.191207
2479.932567	173.764039	47.196212
2477.021915	175.426584	47.201217
2473.597825	176.909044	47.206221
2470.267633	178.333185	47.211226
2466.907750	171.032471	47.216231
2463.452232	174.388348	47.221236
2460.149207	165.709503	47.226241
2456.620468	164.982851	47.231245
2453.388264	175.406726	47.236250
2449.995782	165.292991	47.241255
2446.229093	165.269869	47.246260
2443.387675	166.028631	47.251265
2440.338093	174.808915	47.256269
2436.563847	173.079657	47.261274
2433.260346	172.559362	47.266279
2429.350234	168.143446	47.271284
2426.249318	165.209002	47.276289
2422.976483	168.072382	47.281293
2418.842673	170.072627	47.286298
2415.522965	170.356813	47.291303
2412.451251	167.746919	47.296308
2408.683168	157.038471	47.301313
2404.796430	171.761327	47.306317
2401.533958	164.346114	47.311322
2398.659045	169.573283	47.316327
2395.355885	163.950327	47.321332
2392.194349	157.005697	47.326337
2388.459205	155.235885	47.331341
2384.683783	156.454930	47.336346
2382.059136	149.753810	47.341351
2377.936922	155.951375	47.346356
2374.307065	163.692175	47.351361
2371.275614	159.484705	47.356365
2367.103072	161.311214	47.361370
2363.744673	157.380320	47.366375
2360.789992	159.388833	47.371380
2357.151873	162.900627	47.376385
2353.959498	156.120961	47.381389
2350.355479	158.369678	47.386394
2346.973096	150.824920	47.391399
2343.198606	158.450292	47.396404
2339.729312	151.533220	47.401409
2336.501766	160.678801	47.406413
2332.786192	158.378114	47.411418
2329.283590	147.891931	47.416423
2325.665603	163.518288	47.421428
2321.963605	153.440760	47.426433
2319.441075	154.212071	47.431437
2315.837504	161.397399	47.436442
2312.223683	151.026088	47.441447
2308.426347	162.261448	47.446452
2304.774245	152.225034	47.451457
2301.553387	157.892793	47.456461
2297.881467	160.276095	47.461466
2294.428803	156.791804	47.466471
2291.347348	161.167265	47.471476
2287.845273	155.749113	47.476481
2284.215590	162.375366	47.481485
2280.688742	158.350385	47.486490
2277.282398	151.940395	47.491495
2273.714720	166.834241	47.496500
2270.251987	155.805938	47.501505
2266.734685	157.868713	47.506509
2262.865080	155.999439	47.511514
2260.058765	154.217481	47.516519
2256.366762	161.875670	47.521524
2252.879624	157.071174	47.526529
2249.650517	154.975987	47.531533
2245.501171	169.608896	47.536538
2242.195681	156.543365	47.541543
2238.607565	164.162511	47.546548
2235.388697	169.828407	47.551553
2232.088633	158.119095	47.556557
2228.335660	158.241091	47.561562
2224.961109	149.123915	47.566567
2221.255940	150.830162	47.571572
2217.973450	148.798474	47.576577
2214.664864	147.553747	47.581581
2211.001762	154.446250	47.586586
2207.361589	157.129266	47.591591
2203.950185	154.501000	47.596596
2200.382618	153.375017	47.601601
2197.281024	160.102202	47.606605
2193.188419	155.970400	47.611610
2190.065877	147.854781	47.616615
2186.542684	155.338519	47.621620
2183.178711	153.059623	47.626625
2180.044776	148.949521	47.631629
2176.067646	147.232264	47.636634
2172.911468	147.557695	47.641639
2168.985281	150.750920	47.646644
2165.632571	146.529342	47.651649
2162.109822	151.366697	47.656653
2158.182646	145.766047	47.661658
2154.925488	150.307156	47.666663
2151.485145	157.305793	47.671668
2148.330050	149.056652	47.676673
2144.948177	145.297338	47.681677
2141.095151	147.200336	47.686682
2137.495983	143.279766	47.691687
2133.820688	154.637366	47.696692
2130.622302	147.731179	47.701697
2127.373877	153.234473	47.706701
2123.884408	149.908142	47.711706
2120.418971	143.669654	47.716711
2116.916459	152.175002	47.721716
2112.856274	147.326511	47.726721
2109.545216	146.179751	47.731725
2105.943538	149.492902	47.736730
2102.682698	146.154884	47.741735
2099.305594	151.708846	47.746740
2095.983601	146.310248	47.751745
2092.320011	150.510016	47.756749
2088.445423	150.584910	47.761754
2085.260995	151.162724	47.766759
2081.852256	144.727431	47.771764
2078.075912	144.931549	47.776769
2074.590171	148.838316	47.781773
2071.357575	145.138670	47.786778
2067.924675	148.004630	47.791783
2064.081892	151.918464	47.796788
2060.779845	153.350660	47.801793
2057.455558	144.222951	47.806797
2053.683404	141.982546	47.811802
2050.476629	144.337956	47.816807
2046.915248	148.027727	47.821812
2043.127753	147.044152	47.826817
2039.994210	148.578582	47.831821
2036.235484	143.385355	47.836826
2032.415923	143.500739	47.841831
2029.196422	149.364591	47.846836
2025.697884	140.342253	47.851841
2022.442266	138.055645	47.856845
2018.428903	143.150340	47.861850
2015.261629	136.852239	47.866855
2011.452102	139.272483	47.871860
2008.146156	135.946721	47.876865
2004.875756	139.672334	47.881869
2001.438581	143.966202	47.886874
1998.146697	130.070612	47.891879
1994.370546	141.693596	47.896884
1990.919074	141.072732	47.901889
1987.276518	136.097762	47.906893
1983.419250	139.676794	47.911898
1980.276340	139.758616	47.916903
1976.667912	136.606761	47.921908
1973.376170	137.144550	47.926913
1969.967221	138.264906	47.931917
1966.146484	137.180715	47.936922
1963.107311	132.889353	47.941927
1959.085587	142.881063	47.946932
1955.771432	142.904354	47.951937
1952.265609	136.962562	47.956941
1948.892161	131.583826	47.961946
1945.849784	128.578078	47.966951
1941.881753	144.984317	47.971956
1938.535846	146.561187	47.976961
1934.798635	142.187001	47.981965
1931.015924	147.221174	47.986970
1927.497522	135.015767	47.991975
1924.292151	138.812785	47.996980
1920.832693	135.365817	48.001985
1917.464815	128.134357	48.006989
1913.765792	140.585318	48.011994
1910.577611	131.601610	48.016999
1906.800141	134.293900	48.022004
1903.164809	138.294164	48.027009
1899.769159	132.735211	48.032013
1896.311529	138.263132	48.037018
1892.925702	135.701325	48.042023
1889.122124	128.459759	48.047028
1885.833359	129.312858	48.052033
1882.451550	118.410073	48.057037
1879.049525	137.547958	48.062042
1875.519129	128.339595	48.067047
1871.925443	133.655368	48.072052
1868.414884	128.985094	48.077057
1864.941084	124.688826	48.082061
1861.247685	138.832057	48.087066
1857.557146	133.065897	48.092071
1854.149884	133.040701	48.097076
1850.514945	131.939531	48.102081
1847.352487	137.608371	48.107085
1843.678202	128.097404	48.112090
1840.718506	126.391951	48.117095
1837.097280	135.168093	48.122100
1833.487827	127.484243	48.127105
1830.132321	124.891426	48.132109
1826.324702	129.593916	48.137114
1822.902388	128.440872	48.142119
1819.368610	122.750878	48.147124
1816.000386	131.178378	48.152129
1812.537260	121.948304	48.157133
1808.511595	131.108789	48.162138
1805.034371	116.497853	48.167143
1801.463336	124.293238	48.172148
1797.981982	122.217344	48.177153
1794.954227	126.833064	48.182157
1791.455276	129.698084	48.187162
1787.746997	120.541287	48.192167
1784.438436	127.961009	48.197172
1780.647314	131.516442	48.202177
1777.106275	130.554136	48.207181
1773.468806	132.532322	48.212186
1770.463318	128.842542	48.217191
1766.843031	126.906446	48.222196
1763.421609	131.610307	48.227201
1759.745330	125.478774	48.232205
1756.238721	131.611826	48.237210
1752.810596	124.039188	48.242215
1749.258469	139.934803	48.247220
1745.920531	134.413797	48.252225
1742.438006	130.472103	48.257229
1738.429982	140.156822	48.262234
1735.255996	129.621994	48.267239
1731.880765	133.396478	48.272244
1728.530101	133.885757	48.277249
1725.178210	121.188297	48.282253
1721.199416	127.778467	48.287258
1717.714588	126.314956	48.292263
1714.261795	128.827458	48.297268
1710.512080	138.946292	48.302273
1707.389932	116.458427	48.307277
1703.962150	135.233407	48.312282
1700.273145	124.734954	48.317287
1696.291299	132.330101	48.322292
1693.120545	129.030780	48.327297
1689.587429	125.737258	48.332301
1686.318620	135.858354	48.337306
1682.987232	133.227915	48.342311
1679.420822	126.476612	48.347316
1675.880184	128.546816	48.352321
1671.894480	126.515271	48.357325
1668.434390	128.788455	48.362330
1665.266619	134.791192	48.367335
1662.104653	127.321471	48.372340
1658.309735	126.673924	48.377345
1654.981571	128.161819	48.382349
1651.368682	123.488892	48.387354
1647.843820	128.091123	48.392359
1643.884623	127.037375	48.397364
1640.532732	137.567888	48.402369
1636.940430	124.077257	48.407373
1633.317013	136.323105	48.412378
1630.538937	131.013784	48.417383
1627.098586	130.032588	48.422388
1623.170546	133.610765	48.427393
1619.968121	128.743350	48.432397
1615.879311	130.977187	48.437402
1612.934076	122.262012	48.442407
1609.405171	134.397733	48.447412
1605.581214	127.592350	48.452417
1602.317324	121.299077	48.457421
1598.228829	126.074986	48.462426
1595.141700	127.221761	48.467431
1591.730161	117.087041	48.472436
1588.387075	115.948708	48.477441
1584.868843	118.599001	48.482445
1581.141532	122.801375	48.487450
1577.613588	120.260920	48.492455
1574.089981	119.355289	48.497460
1570.808927	120.231406	48.502465
1567.644816	114.748522	48.507469
1563.351320	120.400176	48.512474
1560.024130	112.536722	48.517479
1556.534828	128.421268	48.522484
1552.926422	124.674972	48.527489
1549.538302	114.685212	48.532493
1545.920338	126.920538	48.537498
1542.502549	112.821979	48.542503
1539.467886	120.961077	48.547508
1535.460126	123.091800	48.552513
1532.443360	123.961963	48.557517
1528.841700	130.390110	48.562522
1525.700147	115.980891	48.567527
1522.219529	121.357355	48.572532
1517.921898	122.827155	48.577537
1514.300600	118.172703	48.582541
1510.747558	121.207297	48.587546
1507.565932	117.975227	48.592551
1503.960630	118.536543	48.597556
1500.820641	118.050658	48.602561
1497.201730	107.799132	48.607565
1493.338258	117.193531	48.612570
1490.154029	115.589546	48.617575
1486.786338	120.793647	48.622580
1483.354026	114.636837	48.627585
1479.799228	122.256296	48.632589
1476.545708	126.386372	48.637594
1472.618784	123.668221	48.642599
1468.857660	125.292918	48.647604
1465.078128	117.736953	48.652609
1462.071848	115.493411	48.657613
1458.533900	121.947386	48.662618
1455.479184	112.190326	48.667623
1451.407151	116.528701	48.672628
1448.051674	115.680828	48.677633
1444.539381	119.212145	48.682637
1440.957539	122.470003	48.687642
1437.682999	122.078031	48.692647
1434.241107	122.139376	48.697652
1430.816298	125.823391	48.702657
1427.378787	110.179686	48.707661
1423.427031	114.799145	48.712666
1420.169430	115.247216	48.717671
1416.449807	123.036437	48.722676
1412.910326	119.628943	48.727681
1409.677110	114.957209	48.732685
1406.036119	123.002216	48.737690
1402.187882	119.950844	48.742695
1398.971968	119.362529	48.747700
1395.858666	119.465501	48.752705
1392.552050	106.362628	48.757709
1388.390418	123.263574	48.762714
1385.142949	112.781240	48.767719
1381.237082	118.583490	48.772724
1377.657043	121.976076	48.777729
1374.396856	107.859319	48.782733
1371.026078	128.333792	48.787738
1367.534668	116.266910	48.792743
1363.990809	123.363670	48.797748
1360.340278	125.713940	48.802753
1357.272736	119.347556	48.807757
1353.387123	129.442720	48.812762
1349.986129	121.998144	48.817767
1346.525127	126.326784	48.822772
1342.858538	122.860631	48.827777
1339.593435	126.289401	48.832781
1336.230965	123.280932	48.837786
1332.539120	128.360917	48.842791
1329.214227	124.904798	48.847796
1325.584295	124.088172	48.852801
1321.996875	126.206627	48.857805
1318.414064	119.838611	48.862810
1314.878690	127.861688	48.867815
1311.544620	119.562070	48.872820
1308.097221	126.137742	48.877825
1304.645702	121.424615	48.882829
1300.818748	123.667141	48.887834
1297.385001	127.744639	48.892839
1293.898148	123.017825	48.897844
1290.054912	121.937519	48.902849
1286.990983	120.610391	48.907853
1283.650082	119.982629	48.912858
1280.127997	115.346508	48.917863
1276.750352	122.203123	48.922868
1272.787690	116.912844	48.927873
1269.213318	118.647926	48.932877
1265.949132	115.145711	48.937882
1262.363821	106.694280	48.942887
1259.065484	114.959214	48.947892
1255.067081	120.544990	48.952897
1251.690962	113.246758	48.957901
1248.169425	124.023406	48.962906
1245.126975	119.326378	48.967911
1241.897951	120.680561	48.972916
1238.134783	123.920198	48.977921
1234.592078	110.753474	48.982925
1230.788770	124.743187	48.987930
1227.325848	113.647162	48.992935
1224.087543	120.292912	48.997940
1220.190166	116.113160	49.002945
1216.780087	105.175559	49.007949
1213.319038	119.656704	49.012954
1209.895043	105.861006	49.017959
1206.532304	115.553106	49.022964
1202.679356	120.517341	49.027969
1199.577231	114.951075	49.032973
1195.774704	116.570600	49.037978
1192.106865	108.319555	49.042983
1189.130760	108.663431	49.047988
1185.299838	110.594321	49.052993
1182.382744	106.102568	49.057997
1178.212255	111.916954	49.063002
1174.477215	120.587246	49.068007
1171.370198	109.417831	49.073012
1167.944091	116.292592	49.078017
1164.617194	121.142459	49.083021
1160.757670	114.510706	49.088026
1157.131171	108.670434	49.093031
1153.586189	104.527207	49.098036
1150.076158	117.441935	49.103041
1146.821672	105.513101	49.108045
1143.526114	119.945023	49.113050
1139.972028	106.436512	49.118055
1136.321734	110.343508	49.123060
1132.919940	113.331668	49.128065
1129.186502	108.299435	49.133069
1125.645834	113.984674	49.138074
1122.023622	114.233937	49.143079
1119.152927	108.570663	49.148084
1115.486515	118.723688	49.153089
1112.165500	111.315227	49.158093
1108.024594	110.579313	49.163098
1104.671651	110.339667	49.168103
1101.519395	107.310440	49.173108
1097.673060	110.993539	49.178113
1094.275952	111.940291	49.183117
1090.437669	112.908485	49.188122
1087.523535	110.384743	49.193127
1083.920424	105.061441	49.198132
1080.236037	112.344236	49.203137
1076.793338	101.091678	49.208141
1073.108397	116.996611	49.213146
1070.066160	105.480702	49.218151
1066.489508	114.719457	49.223156
1062.593219	110.166505	49.228161
1058.951535	108.494215	49.233165
1055.536084	111.336488	49.238170
1052.253884	116.041299	49.243175
1048.841462	112.076337	49.248180
1045.232102	111.299358	49.253185
1041.990943	105.080521	49.258189
1038.211502	117.328272	49.263194
1034.916390	117.159234	49.268199
1031.568188	108.606243	49.273204
1027.459240	119.127919	49.278209
1024.356515	114.271309	49.283213
1020.409128	124.472050	49.288218
1017.299810	116.044934	49.293223
1013.671786	114.212946	49.298228
1010.458206	118.605500	49.303233
1006.808769	111.651040	49.308237
1003.109660	120.670328	49.313242
999.574079	112.559202	49.318247
996.241200	114.918598	49.323252
992.638329	113.966932	49.328257
989.291348	116.268478	49.333261
985.521547	117.375806	49.338266
981.744632	108.647475	49.343271
978.561753	106.538650	49.348276
975.084023	116.076060	49.353281
972.154400	117.065774	49.358285
968.094369	118.074885	49.363290
964.385860	121.744774	49.368295
960.980949	116.597382	49.373300
957.422723	121.974054	49.378305
954.564266	112.891589	49.383309
950.984055	117.863611	49.388314
947.105361	114.121473	49.393319
943.783483	107.251826	49.398324
939.940712	118.824574	49.403329
936.661823	109.214710	49.408333
932.933449	108.948281	49.413338
929.800521	104.156138	49.418343
926.353669	109.252939	49.423348
922.742228	109.703245	49.428353
919.249023	104.817953	49.433357
915.272485	113.480616	49.438362
911.686205	113.909601	49.443367
908.445057	113.386590	49.448372
905.208446	117.326978	49.453377
901.908670	114.074439	49.458381
898.203847	116.992115	49.463386
894.440917	112.635516	49.468391
891.346068	98.657607	49.473396
887.763689	111.424227	49.478401
884.120837	109.093960	49.483405
880.562743	119.022429	49.488410
876.611209	112.643357	49.493415
873.306635	115.544191	49.498420
869.963681	110.023923	49.503425
866.846607	108.525117	49.508429
863.128931	106.010302	49.513434
859.674139	110.409105	49.518439
856.098541	102.468716	49.523444
852.269630	106.206557	49.528449
848.697058	107.723018	49.533453
845.720626	109.729338	49.538458
842.409311	116.330971	49.543463
838.796073	102.671896	49.548468
835.235746	105.804894	49.553473
831.629758	100.657718	49.558477
827.796023	106.646405	49.563482
824.452501	99.764653	49.568487
821.332551	104.486985	49.573492
817.564340	113.512111	49.578497
813.912845	103.994373	49.583501
810.503633	107.757157	49.588506
806.831073	103.882583	49.593511
803.156465	103.228287	49.598516
799.688887	105.979320	49.603521
796.729510	110.697804	49.608525
793.124652	105.838584	49.613530
789.747965	101.715185	49.618535
786.047570	106.152100	49.623540
782.133140	110.836757	49.628545
779.176406	102.845377	49.633549
775.437712	103.514187	49.638554
772.058165	95.731482	49.643559
768.752436	97.574068	49.648564
764.880407	101.850341	49.653569
761.498927	104.208275	49.658573
757.814299	107.008662	49.663578
754.231629	103.934658	49.668583
750.700764	101.140200	49.673588
747.379831	98.055073	49.678593
744.343038	98.282790	49.683597
740.757873	110.964720	49.688602
737.229098	111.032680	49.693607
733.583169	100.751986	49.698612
729.737008	108.744387	49.703617
726.361495	97.789665	49.708621
722.903534	101.267531	49.713626
719.601196	98.412404	49.718631
716.005736	105.149331	49.723636
712.286971	108.157671	49.728641
709.114393	105.119270	49.733645
705.709093	103.147885	49.738650
701.523190	98.993846	49.743655
698.434853	104.060116	49.748660
694.917536	109.401401	49.753665
691.267807	92.576535	49.758669
687.764341	105.715035	49.763674
684.578840	101.428273	49.768679
680.929919	102.801206	49.773684
677.113496	109.044082	49.778689
673.616593	102.236767	49.783693
670.112150	105.837410	49.788698
666.761617	93.437467	49.793703
663.690490	94.053948	49.798708
659.872026	101.071716	49.803713
656.598850	107.177374	49.808717
652.672544	108.884133	49.813722
649.381268	108.443805	49.818727
645.994740	95.195764	49.823732
642.740496	99.158979	49.828737
639.024466	93.163284	49.833741
635.219678	103.376240	49.838746
631.922507	102.581302	49.843751
628.177230	99.861096	49.848756
624.843273	98.860113	49.853761
621.316792	102.202969	49.858765
617.742334	99.264477	49.863770
614.116370	111.118315	49.868775
610.813770	100.066183	49.873780
607.345258	105.989886	49.878785
603.981820	103.105095	49.883789
600.609267	107.391419	49.888794
596.887305	102.282186	49.893799
593.267992	98.458784	49.898804
589.496846	111.494034	49.903809
586.321814	103.366250	49.908813
582.807546	104.299224	49.913818
579.394284	108.663340	49.918823
575.765793	106.307477	49.923828
572.165780	112.555678	49.928833
568.920145	109.410081	49.933837
565.134830	112.157822	49.938842
561.746261	101.441219	49.943847
558.526412	98.325505	49.948852
554.852262	110.169005	49.953857
551.338270	105.394418	49.958861
547.787293	109.302805	49.963866
544.098695	101.371527	49.968871
540.416494	110.000588	49.973876
537.174048	121.680324	49.978881
533.610786	103.115992	49.983885
530.448871	107.764158	49.988890
526.800118	103.508586	49.993895
523.420978	104.489500	49.998900
519.671851	107.452700	50.003905
516.210265	101.302924	50.008909
512.813967	99.095573	50.013914
509.528822	94.654544	50.018919
505.928417	93.633806	50.023924
502.358475	112.454263	50.028929
498.940204	99.708101	50.033933
495.139326	109.269116	50.038938
491.399004	101.741118	50.043943
488.084670	94.855016	50.048948
484.370700	102.126180	50.053953
481.261028	100.942560	50.058957
477.794597	106.341890	50.063962
474.136473	104.179474	50.068967
470.757862	95.815126	50.073972
467.314033	102.066369	50.078977
463.609012	104.625278	50.083981
460.224311	100.350341	50.088986
456.657207	100.586686	50.093991
453.180247	104.415013	50.098996
449.514240	98.639133	50.104001
446.257704	97.538847	50.109005
443.109637	98.520063	50.114010
439.274681	100.194133	50.119015
435.591070	101.508085	50.124020
432.275895	95.272586	50.129025
428.582219	95.879183	50.134029
424.814970	90.310710	50.139034
421.408415	94.502345	50.144039
418.172111	95.914756	50.149044
414.566988	95.947660	50.154049
411.325338	93.478785	50.159053
407.520939	111.283343	50.164058
404.529253	103.409133	50.169063
400.822597	102.310162	50.174068
396.744775	106.039059	50.179073
393.564721	106.867934	50.184077
390.133329	105.410245	50.189082
386.592937	108.213111	50.194087
383.285205	106.063627	50.199092
379.672035	110.261667	50.204097
376.202121	100.792434	50.209101
372.416120	106.467523	50.214106
368.454100	102.018059	50.219111
365.805240	95.661484	50.224116
361.865264	101.288063	50.229121
358.599248	95.112176	50.234125
355.287840	95.822711	50.239130
351.741076	103.437689	50.244135
348.279605	96.443053	50.249140
344.331398	104.737403	50.254145
341.027709	96.729982	50.259149
337.694376	100.583169	50.264154
334.312177	98.821184	50.269159
330.813135	94.835039	50.274164
326.936281	102.276945	50.279169
323.556422	98.089925	50.284173
319.938203	92.457217	50.289178
316.424508	95.745109	50.294183
313.182773	93.476817	50.299188
309.545466	97.721924	50.304193
306.421178	90.308223	50.309197
302.817789	96.697488	50.314202
298.909636	99.999970	50.319207
295.756047	94.526391	50.324212
291.791795	92.769220	50.329217
288.534414	88.655298	50.334221
284.794412	98.314336	50.339226
281.461790	90.092520	50.344231
277.854409	87.312114	50.349236
274.396948	93.147006	50.354241
270.796985	94.880203	50.359245
267.596539	102.594405	50.364250
263.836542	98.896996	50.369255
260.909738	90.468507	50.374260
257.286179	103.410496	50.379265
253.729861	95.742352	50.384269
249.994133	99.272673	50.389274
246.145930	96.152681	50.394279
242.947257	86.029310	50.399284
239.444511	89.355902	50.404289
235.889754	86.446447	50.409293
232.571991	94.123059	50.414298
229.038206	90.384095	50.419303
225.691430	88.765520	50.424308
221.845341	90.150948	50.429313
218.301179	93.507107	50.434317
214.821640	95.560028	50.439322
211.233939	89.410680	50.444327
208.017157	91.872400	50.449332
204.441788	105.658740	50.454337
200.960396	97.185151	50.459341
197.407723	99.528830	50.464346
193.874079	102.754606	50.469351
190.443471	95.587069	50.474356
186.841094	107.006915	50.479361
183.577755	93.822186	50.484365
180.009618	98.542770	50.489370
176.261061	96.424003	50.494375
172.738750	88.259733	50.499380
169.201225	98.619228	50.504385
165.895072	97.538027	50.509389
162.653945	102.979621	50.514394
159.327170	94.620779	50.519399
155.629300	97.180142	50.524404
151.559174	104.773183	50.529409
148.265402	98.728555	50.534413
144.929821	101.096918	50.539418
141.198705	102.033194	50.544423
137.768175	94.750841	50.549428
133.993547	98.186466	50.554433
130.924104	98.106057	50.559437
127.406672	90.205448	50.564442
123.802700	98.214869	50.569447
120.536720	92.298472	50.574452
117.000324	95.864574	50.579457
113.874402	92.734251	50.584461
109.897755	94.065617	50.589466
106.042406	97.592183	50.594471
102.849726	85.565240	50.599476
99.294695	92.492284	50.604481
95.642735	91.109442	50.609485
92.404745	87.579342	50.614490
88.720588	94.906262	50.619495
85.479628	84.721751	50.624500
81.500108	97.325957	50.629505
78.216368	91.884758	50.634509
74.789735	88.135686	50.639514
71.332465	92.373868	50.644519
68.187500	92.985037	50.649524
64.360259	91.169482	50.654529
61.084857	100.936671	50.659533
57.315499	95.442496	50.664538
53.623671	94.435110	50.669543
50.157212	89.905090	50.674548
46.832225	91.918939	50.679553
43.297032	87.984417	50.684557
40.042961	94.822602	50.689562
35.974919	100.717138	50.694567
33.017012	90.184077	50.699572
29.172938	97.167522	50.704577
25.962427	86.850937	50.709581
22.214170	91.807289	50.714586
18.933534	95.867474	50.719591
15.481578	90.097204	50.724596
11.389715	100.045994	50.729601
8.137587	93.516055	50.734605
4.712135	93.634402	50.739610
0.762589	89.734390	50.744615