Tue Jun 21 10:55:44 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.422058	72.471372	0.000000
0.195869	70.256125	0.005005
0.368402	80.441625	0.010010
0.400898	80.036903	0.015014
-0.077621	72.775773	0.020019
0.604443	76.084663	0.025024
0.126485	70.529986	0.030029
0.116188	51.545083	0.035034
-0.436611	43.051092	0.040038
-0.843170	31.913091	0.045043
-0.971004	21.943727	0.050048
-1.418856	26.390067	0.055053
-1.586441	11.451730	0.060058
-1.633637	8.424821	0.065062
-2.250171	-0.652367	0.070067
-2.319159	-3.901019	0.075072
-2.955051	1.655272	0.080077
-3.488910	-10.592731	0.085082
-3.728131	-2.641583	0.090086
-4.101671	-6.588287	0.095091
-3.777978	-10.987886	0.100096
-4.126457	-4.645656	0.105101
-4.530254	-6.532127	0.110106
-4.919049	-5.577711	0.115110
-5.606836	-6.071936	0.120115
-5.261685	-11.988829	0.125120
-5.492881	-0.214105	0.130125
-5.498436	-14.875749	0.135130
-6.140140	-15.517316	0.140134
-6.898027	-14.300503	0.145139
-6.989840	-6.931626	0.150144
-7.181474	-8.434489	0.155149
-7.156555	-12.062374	0.160154
-6.888852	-3.546734	0.165158
-7.418264	-3.337447	0.170163
-7.540791	-9.515520	0.175168
-8.267822	-7.740232	0.180173
-8.689499	-3.612585	0.185178
-8.728346	-3.306933	0.190182
-9.114999	-0.151227	0.195187
-9.130171	-8.871756	0.200192
-8.873009	-7.400932	0.205197
-9.399529	-9.645170	0.210202
-10.052361	-15.456002	0.215206
-10.406235	2.276390	0.220211
-10.170981	-8.123670	0.225216
-10.353242	-14.554696	0.230221
-10.749523	-11.826400	0.235226
-10.791743	-9.925740	0.240230
-11.907152	-10.271403	0.245235
-11.751160	-7.959961	0.250240
-11.704077	-0.109502	0.255245
-11.892921	-5.513113	0.260250
-11.942520	-21.513070	0.265254
-12.810209	-7.927602	0.270259
-13.191446	-14.561887	0.275264
-13.675500	-4.749801	0.280269
-13.878037	-3.143653	0.285274
-13.636418	-11.689834	0.290278
-13.831132	-1.164547	0.295283
-13.435518	-11.340152	0.300288
-13.848115	-10.723970	0.305293
-14.560973	-14.402743	0.310298
-14.686573	-9.524928	0.315302
-14.963164	-9.164909	0.320307
-14.771483	-12.356875	0.325312
-15.629956	-14.950673	0.330317
-16.052650	-12.451447	0.335322
-15.988508	-5.522203	0.340326
-16.279679	-4.161265	0.345331
-16.563749	-7.165719	0.350336
-17.388996	-8.636473	0.355341
-17.831626	-13.633383	0.360346
-17.776254	-5.242424	0.365350
-17.946106	-12.885551	0.370355
-18.183700	-8.329786	0.375360
-18.156852	-5.934207	0.380365
-17.872120	-3.114639	0.385370
-17.946360	-7.661463	0.390374
-18.502516	-9.061732	0.395379
-19.374316	-8.372862	0.400384
-19.864742	-6.774294	0.405389
-20.041175	-1.886875	0.410394
-19.743969	-18.291175	0.415398
-19.966310	-9.358924	0.420403
-19.765433	-16.585303	0.425408
-20.699172	-8.003715	0.430413
-21.414551	-6.220093	0.435418
-21.221004	-3.622423	0.440422
-21.401330	-5.297850	0.445427
-21.415899	-13.970128	0.450432
-21.458667	-10.595696	0.455437
-22.032937	-11.057410	0.460442
-22.641387	-16.290693	0.465446
-22.867722	-8.970582	0.470451
-22.937041	-18.413454	0.475456
-23.179260	-2.364849	0.480461
-23.141010	-5.422086	0.485466
-23.631408	-0.654552	0.490470
-23.978305	-7.513564	0.495475
-24.252382	-6.785738	0.500480
-24.601571	1.974138	0.505485
-24.512914	-9.072576	0.510490
-24.377948	1.111393	0.515494
-25.580363	-8.836484	0.520499
-25.667016	-8.632633	0.525504
-26.167737	-4.510642	0.530509
-26.138307	-4.110921	0.535514
-25.977082	-9.749507	0.540518
-26.378803	-1.280288	0.545523
-26.443263	-5.620348	0.550528
-26.475074	-10.856574	0.555533
-27.302661	-5.194144	0.560538
-27.412912	-10.136378	0.565542
-27.883099	0.136949	0.570547
-27.755199	-7.100239	0.575552
-28.065865	-4.929376	0.580557
-28.319465	-5.818729	0.585562
-28.596499	-1.557759	0.590566
-29.112624	-8.276266	0.595571
-29.300413	-14.607511	0.600576
-29.226196	-7.614029	0.605581
-29.361207	-1.562693	0.610586
-29.604334	-7.452026	0.615590
-30.323829	-2.571370	0.620595
-30.400170	-15.749578	0.625600
-30.857569	0.404912	0.630605
-30.786884	-2.270332	0.635610
-30.421984	-7.827996	0.640614
-31.520095	-2.552136	0.645619
-31.974010	-7.009643	0.650624
-32.230989	-0.532787	0.655629
-32.187913	-6.432220	0.660634
-32.254351	-3.938707	0.665638
-32.621811	-3.260142	0.670643
-32.622819	-8.510546	0.675648
-33.674339	-7.659698	0.680653
-33.786242	-6.258788	0.685658
-33.743351	-11.878369	0.690662
-34.167423	-8.819277	0.695667
-33.894950	-6.957706	0.700672
-34.180476	-8.351680	0.705677
-34.616482	-12.452610	0.710682
-35.214075	-8.503623	0.715686
-35.420840	-7.803519	0.720691
-35.524188	-5.301329	0.725696
-36.046806	-11.096227	0.730701
-35.341310	-10.916206	0.735706
-35.417640	-15.480835	0.740710
-36.581744	-6.986205	0.745715
-37.061994	-10.825643	0.750720
-37.379606	-10.566574	0.755725
-37.388918	-3.236816	0.760730
-37.432208	-6.733033	0.765734
-37.529041	-5.474725	0.770739
-37.439075	-3.815191	0.775744
-38.213170	-7.223933	0.780749
-38.854959	-2.116384	0.785754
-38.516587	-8.727558	0.790758
-39.034183	-1.666655	0.795763
-38.805866	-11.839814	0.800768
-39.020695	-5.623710	0.805773
-39.991113	-4.575145	0.810778
-40.398286	-5.687705	0.815782
-40.604365	-0.265735	0.820787
-40.699474	-5.769719	0.825792
-40.715812	5.495630	0.830797
-40.571137	-0.649535	0.835802
-40.632482	-10.979952	0.840806
-41.111245	0.200554	0.845811
-41.946077	-2.861875	0.850816
-42.000273	-3.253423	0.855821
-42.618661	-10.575209	0.860826
-42.154192	-17.814257	0.865830
-42.770659	-11.429426	0.870835
-42.200944	-18.688862	0.875840
-43.075979	-10.994335	0.880845
-43.457053	-12.978691	0.885850
-43.412567	-16.224621	0.890854
-44.201170	-6.877733	0.895859
-44.739983	-17.169726	0.900864
-45.272067	-10.494778	0.905869
-44.586001	-8.094507	0.910874
-44.549929	-13.291653	0.915878
-45.168793	-5.498453	0.920883
-45.073654	-9.765682	0.925888
-45.501117	-8.874913	0.930893
-46.295781	-1.831865	0.935898
-46.467008	-4.791857	0.940902
-46.784864	-7.651000	0.945907
-46.721642	-8.932625	0.950912
-46.617041	-8.366964	0.955917
-46.850664	-6.570175	0.960922
-47.213575	-14.652754	0.965926
-48.105885	-7.586237	0.970931
-48.065157	-15.365464	0.975936
-48.617078	-6.098026	0.980941
-48.780063	-3.009551	0.985946
-48.442752	-7.722404	0.990950
-48.385068	-11.476876	0.995955
-48.877199	-14.197835	1.000960
-49.874177	-5.730484	1.005965
-50.335416	-10.519477	1.010970
-50.169416	-10.646361	1.015974
-50.232340	-9.631059	1.020979
-50.161288	-8.399961	1.025984
-49.880618	-12.927807	1.030989
-50.904530	-8.373051	1.035994
-51.366247	-7.640592	1.040998
-51.943227	-1.284791	1.046003
-51.770036	-16.143564	1.051008
-51.795768	-12.051887	1.056013
-51.905423	-6.369819	1.061018
-52.743873	-10.259652	1.066022
-53.359374	-3.043417	1.071027
-53.250148	-9.172446	1.076032
-53.358607	-4.661549	1.081037
-53.244418	-9.682389	1.086042
-53.135884	-6.774249	1.091046
-53.790885	-6.805230	1.096051
-54.525981	-9.762022	1.101056
-54.850068	-13.701515	1.106061
-55.119755	-2.934713	1.111066
-54.822774	-13.656972	1.116070
-55.179085	-8.070217	1.121075
-55.021528	-11.705858	1.126080
-55.241423	-6.091571	1.131085
-56.096311	-9.971578	1.136090
-56.242447	-1.089635	1.141094
-56.336052	-1.191089	1.146099
-56.390508	3.610814	1.151104
-57.314106	-10.854196	1.156109
-57.883193	-11.953753	1.161114
-57.388647	-14.027467	1.166118
-57.966521	-5.008711	1.171123
-57.391075	-11.762744	1.176128
-57.762278	-6.608246	1.181133
-58.618129	-12.525159	1.186138
-58.921780	-10.034198	1.191142
-59.427723	-9.033935	1.196147
-59.458451	-9.190400	1.201152
-59.721187	-12.140563	1.206157
-59.641228	-4.282136	1.211162
-59.546436	-8.355329	1.216166
-59.696929	-0.536881	1.221171
-60.257183	-4.464892	1.226176
-60.744648	0.812857	1.231181
-61.232720	-15.350691	1.236186
-61.034905	-6.829407	1.241190
-61.583401	-6.201765	1.246195
-61.948469	-7.452719	1.251200
-62.305856	-2.130209	1.256205
-62.528846	-3.952883	1.261210
-62.707907	-12.907729	1.266214
-62.823569	-5.782954	1.271219
-62.684121	-8.829321	1.276224
-62.634293	-8.674711	1.281229
-63.515337	-10.886868	1.286234
-64.074489	-4.964601	1.291238
-64.672567	-6.512037	1.296243
-64.382157	-7.623101	1.301248
-64.298839	-8.053406	1.306253
-64.789439	-4.396623	1.311258
-64.610595	-10.906983	1.316262
-65.010024	-5.453389	1.321267
-65.640806	-7.603787	1.326272
-66.078014	-11.358787	1.331277
-66.194110	-8.683201	1.336282
-66.283727	-14.178815	1.341286
-66.373904	-12.437355	1.346291
-66.242705	-2.350055	1.351296
-67.465098	-6.174131	1.356301
-67.786650	-9.444099	1.361306
-67.576676	-14.244396	1.366310
-67.742954	-3.583519	1.371315
-68.144244	-11.593240	1.376320
-67.921541	-11.081079	1.381325
-68.244197	-4.690042	1.386330
-68.419856	-10.802873	1.391334
-69.332919	6.471960	1.396339
-69.499550	-14.276373	1.401344
-69.301377	-5.673059	1.406349
-69.725682	-3.405427	1.411354
-69.205730	-15.911203	1.416358
-70.211252	-7.094734	1.421363
-70.848087	-9.629322	1.426368
-70.934459	-9.176877	1.431373
-71.322275	-8.516249	1.436378
-70.890841	-5.755910	1.441382
-71.391807	-7.769742	1.446387
-72.032887	-12.810739	1.451392
-72.654688	-3.929549	1.456397
-72.761152	-5.299302	1.461402
-72.784955	-4.763091	1.466406
-73.041814	-3.168271	1.471411
-72.760594	-6.349216	1.476416
-72.631082	1.173828	1.481421
-72.785407	-11.699212	1.486426
-73.389844	-10.595217	1.491430
-74.330553	-5.380542	1.496435
-74.630171	-1.930815	1.501440
-74.739275	-12.715667	1.506445
-74.565403	-4.999286	1.511450
-74.592981	-8.008718	1.516454
-75.659840	0.188028	1.521459
-76.155288	-5.054689	1.526464
-75.853787	-5.427986	1.531469
-76.225129	3.193479	1.536474
-75.813887	-7.556389	1.541478
-76.009292	-8.019665	1.546483
-76.767852	-2.432003	1.551488
-76.849442	-5.705599	1.556493
-77.710492	-5.194912	1.561498
-77.626628	-4.864590	1.566502
-77.956460	-9.615747	1.571507
-77.703281	-5.144218	1.576512
-78.010439	0.155767	1.581517
-78.752013	0.465713	1.586522
-78.904945	-8.438602	1.591526
-79.417126	2.741518	1.596531
-79.500701	-2.953221	1.601536
-79.487659	2.775426	1.606541
-79.655649	-3.439514	1.611546
-79.608882	-6.002854	1.616550
-80.301265	1.246838	1.621555
-80.838671	-11.638731	1.626560
-80.873188	-2.854604	1.631565
-81.184975	0.522745	1.636570
-80.915475	-10.158853	1.641574
-81.505644	5.470621	1.646579
-82.198250	4.124729	1.651584
-82.003828	-5.570798	1.656589
-82.528667	4.998506	1.661594
-82.264447	-8.228208	1.666598
-82.333331	-2.957029	1.671603
-82.894400	6.283319	1.676608
-83.451279	5.025849	1.681613
-83.863789	0.657395	1.686618
-83.416025	-2.843974	1.691622
-84.137826	3.959488	1.696627
-83.972215	-4.572528	1.701632
-84.491705	-8.489525	1.706637
-85.296251	10.927938	1.711642
-85.208309	-3.551263	1.716646
-85.463723	0.356257	1.721651
-85.247117	-6.221136	1.726656
-85.088634	1.155423	1.731661
-85.975235	-3.319218	1.736666
-86.329145	-5.105211	1.741670
-86.841147	2.963733	1.746675
-86.992292	-6.720344	1.751680
-86.940744	1.037807	1.756685
-86.778513	-4.932268	1.761690
-87.392866	-6.296249	1.766694
-87.999844	3.209416	1.771699
-88.560093	-5.055177	1.776704
-88.374114	-8.996854	1.781709
-88.498541	-0.703599	1.786714
-88.532626	-4.071494	1.791718
-89.211322	3.896790	1.796723
-89.823704	6.268389	1.801728
-89.916977	6.332048	1.806733
-90.415150	11.671959	1.811738
-90.380098	-5.410183	1.816742
-90.467812	10.189954	1.821747
-90.464237	7.579696	1.826752
-90.431500	-1.841402	1.831757
-90.726637	2.209449	1.836762
-90.595404	-5.993049	1.841766
-91.494784	-0.005354	1.846771
-91.748515	0.407321	1.851776
-91.905927	0.223885	1.856781
-92.421437	0.537045	1.861786
-93.098874	-7.751552	1.866790
-93.361098	8.408507	1.871795
-93.584929	-5.173486	1.876800
-93.248071	1.206206	1.881805
-93.346222	5.149448	1.886810
-93.596523	7.077664	1.891814
-93.960107	1.127773	1.896819
-93.917863	-1.616168	1.901824
-94.476206	-0.601105	1.906829
-95.110336	-1.025071	1.911834
-95.389705	-7.437443	1.916838
-95.454160	-7.910171	1.921843
-95.163150	-0.746580	1.926848
-95.053994	-7.765963	1.931853
-96.092449	4.543235	1.936858
-96.217091	-5.035710	1.941862
-96.712869	-7.129134	1.946867
-96.814411	1.635114	1.951872
-96.634094	3.384072	1.956877
-97.702553	3.352703	1.961882
-97.973444	-2.480916	1.966886
-97.981604	9.175372	1.971891
-98.351958	-9.500771	1.976896
-98.355437	-11.963634	1.981901
-98.883999	-5.261046	1.986906
-98.527916	-7.902450	1.991910
-98.525899	4.944631	1.996915
-99.558232	-6.077383	2.006912
-98.873711	-1.687456	2.016909
-98.518620	2.909172	2.026906
-98.304381	1.192758	2.036902
-97.587577	1.454324	2.046899
-97.056922	0.391479	2.056896
-96.884866	5.023362	2.066893
-95.700906	-6.558657	2.076890
-95.445019	-1.007069	2.086886
-95.399072	-1.359340	2.096883
-94.265102	-0.509298	2.106880
-94.019563	-6.462781	2.116877
-93.933364	-1.914486	2.126874
-93.066245	-4.847875	2.136870
-92.477749	4.024971	2.146867
-92.274205	-0.984213	2.156864
-91.416564	1.180092	2.166861
-91.217110	11.965392	2.176858
-90.497497	5.135936	2.186854
-89.876786	6.472278	2.196851
-89.374228	2.278405	2.206848
-89.256353	-5.980703	2.216845
-88.545903	6.205808	2.226842
-88.282258	3.216071	2.236838
-87.108956	5.955633	2.246835
-86.559334	-1.725318	2.256832
-86.667153	2.529884	2.266829
-86.434040	6.785332	2.276826
-85.826323	1.284008	2.286822
-85.144707	4.722454	2.296819
-83.965026	3.906000	2.306816
-83.804860	5.782941	2.316813
-83.362026	4.465531	2.326810
-83.309292	5.351392	2.336806
-83.049034	-1.129317	2.346803
-82.132836	1.624767	2.356800
-81.321747	2.111776	2.366797
-80.936432	1.272762	2.376794
-80.899371	6.394490	2.386790
-79.972383	6.250975	2.396787
-79.460607	-5.466308	2.406784
-79.222065	0.813887	2.416781
-78.041741	3.564143	2.426778
-77.662191	4.752325	2.436774
-78.111813	6.136311	2.446771
-77.173625	-2.315160	2.456768
-76.491029	4.169894	2.466765
-76.052486	-1.172808	2.476762
-75.023533	5.130408	2.486758
-74.847321	0.620307	2.496755
-74.697249	6.607317	2.506752
-74.064670	0.924642	2.516749
-73.075026	-1.328595	2.526746
-72.898384	1.509638	2.536742
-72.796316	-1.336764	2.546739
-72.058749	0.897026	2.556736
-71.286331	6.309136	2.566733
-71.034691	2.997940	2.576730
-70.510502	-1.576506	2.586726
-69.813338	-0.170824	2.596723
-69.558005	-4.275936	2.606720
-69.283726	0.019522	2.616717
-68.423105	1.685227	2.626714
-68.393577	2.549442	2.636710
-67.556006	4.277450	2.646707
-67.041881	5.370437	2.656704
-65.964207	2.554915	2.666701
-65.815062	-5.715300	2.676698
-65.694734	-1.033159	2.686694
-65.259021	4.032626	2.696691
-63.927354	-1.327774	2.706688
-63.738003	-6.535551	2.716685
-63.631252	-5.272158	2.726682
-63.282996	4.353566	2.736678
-62.105868	-5.158792	2.746675
-61.825204	0.357479	2.756672
-61.736365	-3.867459	2.766669
-61.064130	0.496849	2.776666
-60.482470	2.301223	2.786662
-60.122576	1.981922	2.796659
-58.485634	-2.953443	2.806656
-59.189304	2.907619	2.816653
-58.654775	3.835998	2.826650
-58.307277	-3.289061	2.836646
-57.659453	-3.185594	2.846643
-56.960966	1.734326	2.856640
-56.044452	2.945814	2.866637
-55.725302	1.670031	2.876634
-55.456655	4.615730	2.886630
-55.488088	1.875805	2.896627
-54.424325	-3.745298	2.906624
-54.139037	-1.376145	2.916621
-52.927409	4.116363	2.926618
-52.809157	-0.198804	2.936614
-52.598736	-6.919426	2.946611
-52.246405	-8.871308	2.956608
-51.314999	-6.511350	2.966605
-51.127662	-4.168062	2.976602
-49.878848	-0.918381	2.986598
-49.944115	-3.264051	2.996595
-49.672977	-4.397920	3.006592
-49.034632	-3.000672	3.016589
-48.347234	-1.378988	3.026586
-48.279191	-3.517733	3.036582
-47.037070	-0.012453	3.046579
-46.485815	-7.093800	3.056576
-46.087894	-5.798208	3.066573
-46.110963	-3.618056	3.076570
-45.946675	2.305351	3.086566
-44.759497	-3.378077	3.096563
-44.745522	-3.576864	3.106560
-43.827508	-3.898491	3.116557
-43.429898	-1.803415	3.126554
-43.051994	-3.760718	3.136550
-42.061848	0.536919	3.146547
-41.528324	-2.369472	3.156544
-41.605436	-2.451419	3.166541
-41.177813	-1.029943	3.176538
-40.314336	1.322893	3.186534
-39.956943	6.457767	3.196531
-39.501914	-1.325278	3.206528
-38.449445	-2.159775	3.216525
-38.371793	-7.015134	3.226522
-38.325257	2.322293	3.236518
-37.775484	3.288853	3.246515
-37.007093	-3.516860	3.256512
-35.864423	-0.218379	3.266509
-35.462282	-2.080112	3.276506
-35.466304	-7.644121	3.286502
-35.208634	0.143847	3.296499
-34.287430	-1.093917	3.306496
-33.820563	0.405035	3.316493
-33.625266	-6.721492	3.326490
-32.970140	-8.900553	3.336486
-32.448254	-1.810347	3.346483
-31.989888	-2.780598	3.356480
-31.225546	-8.530333	3.366477
-30.676657	-4.270072	3.376474
-30.647444	-4.518013	3.386470
-30.105540	-0.870098	3.396467
-29.363785	-2.461461	3.406464
-28.641545	-3.275847	3.416461
-28.112764	-3.092398	3.426458
-27.599454	1.337358	3.436454
-27.310485	-2.442763	3.446451
-27.299301	-1.930768	3.456448
-26.263474	-3.673771	3.466445
-26.030669	-0.425164	3.476442
-25.477187	-1.178211	3.486438
-24.562673	2.039505	3.496435
-24.335357	-3.029137	3.506432
-24.141381	-4.299205	3.516429
-23.378591	-5.725510	3.526426
-22.932020	-0.305864	3.536422
-22.434723	5.370347	3.546419
-21.259963	-10.046259	3.556416
-21.138577	-1.797872	3.566413
-21.190499	-6.142948	3.576410
-20.585423	-6.331145	3.586406
-19.857734	-4.785284	3.596403
-19.552317	-4.028203	3.606400
-18.510221	-6.238741	3.616397
-18.057294	-2.430470	3.626394
-17.916766	0.176052	3.636390
-17.779662	-7.708460	3.646387
-16.564640	-9.842715	3.656384
-16.287583	-4.506041	3.666381
-16.104787	-0.341838	3.676378
-14.965541	-2.523019	3.686374
-14.667351	-1.041775	3.696371
-14.605418	3.216340	3.706368
-13.934045	-1.389391	3.716365
-13.117445	1.162081	3.726362
-12.736035	-4.725581	3.736358
-12.585462	-9.012707	3.746355
-11.681721	-2.485029	3.756352
-11.169260	-0.533843	3.766349
-11.080534	-7.749024	3.776346
-10.180249	-3.334347	3.786342
-9.584103	-4.652241	3.796339
-9.550669	-2.650183	3.806336
-8.633038	-3.384100	3.816333
-7.966347	-4.060853	3.826330
-7.902725	-1.716241	3.836326
-7.655153	-6.724020	3.846323
-7.095638	-3.087712	3.856320
-6.527175	-6.606275	3.866317
-5.762852	1.925091	3.876314
-5.185405	-6.238223	3.886310
-5.067779	-5.876039	3.896307
-4.353092	2.349386	3.906304
-4.191696	3.756269	3.916301
-3.133806	23.840881	3.926298
-2.942360	28.360105	3.936294
-2.989855	31.059809	3.946291
-2.296041	40.524416	3.956288
-1.756735	66.806696	3.966285
-1.140518	78.005747	3.976282
-0.838219	93.777576	3.986278
-0.287081	114.300890	3.996275
0.000000	113.552586	4.001280
0.112839	145.785950	4.006285
0.252653	139.705865	4.011290
0.269927	136.795338	4.016294
0.587616	162.278528	4.021299
0.816122	164.043211	4.026304
0.818796	167.273009	4.031309
1.260429	174.996853	4.036314
1.317024	174.513150	4.041318
1.114596	174.648952	4.046323
1.058563	165.194097	4.051328
0.907311	168.650666	4.056333
1.033966	168.127143	4.061338
1.125922	175.751220	4.066342
1.047719	169.844569	4.071347
0.722886	156.006818	4.076352
0.681151	165.798257	4.081357
0.656418	169.325243	4.086362
1.091997	179.188613	4.091366
1.077689	180.024786	4.096371
1.345424	182.757417	4.101376
1.238382	185.070018	4.106381
1.214642	172.070206	4.111386
1.099757	176.357457	4.116390
1.184993	193.205122	4.121395
1.132665	180.054735	4.126400
1.030776	176.795705	4.131405
1.088600	176.048356	4.136410
0.926800	174.393520	4.141414
0.880282	176.730631	4.146419
0.954864	179.357111	4.151424
1.119020	180.822438	4.156429
0.962323	180.064829	4.161434
0.941782	180.115653	4.166438
0.962158	202.230491	4.171443
1.740052	202.575149	4.176448
1.588679	208.452266	4.181453
1.251755	201.106060	4.186458
1.336800	201.623662	4.191462
1.649881	205.645875	4.196467
1.794301	178.526479	4.201472
1.359091	186.180627	4.206477
1.063751	189.020708	4.211482
1.063668	171.819063	4.216486
1.276877	203.153443	4.221491
1.516194	195.250449	4.226496
1.350338	199.420049	4.231501
1.641212	209.604193	4.236506
1.945626	195.756140	4.241510
1.353644	190.370671	4.246515
1.218229	179.739413	4.251520
1.344771	191.852675	4.256525
1.510817	198.124587	4.261530
1.750763	201.414362	4.266534
1.725897	207.380052	4.271539
1.512664	190.326558	4.276544
1.451946	184.134817	4.281549
1.280222	187.286740	4.286554
1.433811	192.936934	4.291558
1.075551	207.371627	4.296563
1.887221	199.689985	4.301568
1.557006	193.363489	4.306573
1.764537	202.299863	4.311578
1.508141	203.981650	4.316582
1.444650	211.900059	4.321587
1.564013	201.969763	4.326592
1.449614	213.510016	4.331597
1.331628	206.515910	4.336602
1.708233	207.615522	4.341606
1.463646	208.344788	4.346611
1.564263	198.691895	4.351616
1.701909	209.322132	4.356621
1.686931	213.089445	4.361626
1.878862	200.917240	4.366630
1.528993	208.710006	4.371635
1.939236	212.219832	4.376640
1.962420	209.942748	4.381645
1.831998	214.119903	4.386650
1.614605	204.646948	4.391654
1.493429	224.858275	4.396659
1.931710	226.796221	4.401664
2.084011	237.273680	4.406669
1.733179	236.298585	4.411674
2.011757	236.986213	4.416678
1.863963	240.316720	4.421683
1.942880	234.778897	4.426688
2.088296	251.533582	4.431693
2.096587	243.698024	4.436698
2.263858	228.298502	4.441702
1.761088	222.617045	4.446707
1.619615	226.277829	4.451712
1.900773	240.316192	4.456717
2.054607	247.194586	4.461722
1.866612	256.461312	4.466726
2.029136	249.214126	4.471731
2.061955	245.443184	4.476736
2.328600	249.510395	4.481741
2.118142	254.459967	4.486746
2.286459	235.878414	4.491750
1.849114	246.766100	4.496755
2.096070	246.787232	4.501760
2.058698	245.172761	4.506765
1.893200	246.562834	4.511770
2.387639	237.244113	4.516774
2.078075	248.528993	4.521779
2.143005	241.810058	4.526784
2.271262	250.685981	4.531789
2.046702	249.194662	4.536794
2.105872	243.851719	4.541798
1.989011	241.544737	4.546803
2.108589	249.506654	4.551808
2.397858	248.700256	4.556813
1.955784	241.504052	4.561818
2.261525	245.782449	4.566822
2.119234	248.765525	4.571827
2.129262	244.369052	4.576832
2.261197	252.785166	4.581837
2.508426	247.279260	4.586842
2.374557	241.336808	4.591846
2.434749	252.982565	4.596851
2.450951	242.109680	4.601856
2.423950	246.195323	4.606861
2.275469	248.009614	4.611866
2.622991	240.761200	4.616870
2.550217	238.773509	4.621875
2.591733	235.889143	4.626880
2.760644	239.100704	4.631885
2.416614	253.703779	4.636890
2.467014	245.348568	4.641894
2.486859	246.853979	4.646899
2.354305	242.434152	4.651904
2.132836	245.209913	4.656909
2.442185	250.733893	4.661914
2.423493	243.509415	4.666918
2.577856	250.545394	4.671923
2.511770	244.175929	4.676928
2.580473	239.091695	4.681933
2.151309	235.985120	4.686938
2.594604	234.164366	4.691942
2.356323	239.398955	4.696947
2.522672	235.945717	4.701952
2.823544	245.684618	4.706957
2.551276	242.329072	4.711962
2.629918	238.164950	4.716966
2.340578	251.407017	4.721971
2.620736	257.373919	4.726976
3.030835	264.941609	4.731981
2.809077	264.956291	4.736986
2.623291	255.854786	4.741990
2.593131	262.171251	4.746995
2.860716	263.857051	4.752000
2.837282	265.414624	4.757005
2.940212	263.444801	4.762010
3.087063	250.222496	4.767014
2.393228	245.099556	4.772019
2.645859	250.265882	4.777024
2.817676	263.457250	4.782029
2.586935	266.536673	4.787034
3.045029	266.584412	4.792038
2.509015	267.481523	4.797043
2.487513	268.031176	4.802048
2.784546	271.121873	4.807053
2.410292	267.917201	4.812058
2.986686	273.459326	4.817062
2.721921	272.477279	4.822067
2.827092	271.904818	4.827072
3.118686	268.856686	4.832077
2.881787	276.790621	4.837082
3.037325	272.138965	4.842086
2.800268	264.332579	4.847091
3.141767	270.366289	4.852096
3.055403	269.153023	4.857101
2.900763	280.617700	4.862106
3.221621	274.777933	4.867110
3.004238	270.082257	4.872115
3.073852	267.134623	4.877120
2.975032	270.089981	4.882125
2.873006	275.667091	4.887130
3.219839	268.186909	4.892134
2.885503	283.443169	4.897139
2.981460	271.582608	4.902144
2.954418	271.896770	4.907149
3.088926	284.087128	4.912154
2.969630	274.919939	4.917158
2.804648	290.547769	4.922163
3.170107	299.910542	4.927168
3.160035	300.720959	4.932173
3.092960	301.602778	4.937178
3.092463	300.688661	4.942182
3.061708	302.154109	4.947187
3.318556	302.530981	4.952192
3.418377	302.715008	4.957197
3.336639	309.832341	4.962202
3.687891	300.133541	4.967206
3.324456	306.740634	4.972211
3.644248	302.518012	4.977216
3.390943	290.244032	4.982221
3.084441	295.607943	4.987226
3.272346	292.733464	4.992230
3.247132	306.897806	4.997235
3.436521	307.847469	5.002240
3.704464	303.878328	5.007245
3.341045	307.266657	5.012250
3.533857	299.834460	5.017254
3.142611	300.638928	5.022259
3.285629	302.491192	5.027264
3.110032	305.437761	5.032269
3.087079	303.390899	5.037274
3.041530	308.413230	5.042278
3.221596	301.755717	5.047283
3.768523	304.644408	5.052288
3.638439	304.470845	5.057293
3.326277	307.222957	5.062298
3.831179	304.112264	5.067302
3.654968	307.667719	5.072307
3.650086	306.686444	5.077312
3.320657	301.401514	5.082317
3.439293	311.112616	5.087322
3.493046	307.267152	5.092326
3.296793	316.579288	5.097331
3.068821	315.141809	5.102336
3.203784	321.209740	5.107341
3.408983	330.486192	5.112346
3.945813	333.333541	5.117350
3.692316	338.608374	5.122355
3.934091	337.213877	5.127360
3.976178	330.588278	5.132365
3.438907	326.354438	5.137370
4.035222	329.842754	5.142374
3.732542	321.424607	5.147379
3.733439	316.481621	5.152384
3.688096	310.004302	5.157389
3.726668	312.220782	5.162394
3.778387	325.838802	5.167398
3.757029	333.201106	5.172403
3.719099	329.556316	5.177408
3.740243	330.691513	5.182413
3.579468	338.026388	5.187418
3.983080	327.937644	5.192422
4.026541	340.324871	5.197427
3.869348	345.749325	5.202432
3.680118	344.739965	5.207437
3.773194	349.071564	5.212442
3.762555	329.325444	5.217446
3.689529	340.821446	5.222451
3.921479	337.694375	5.227456
4.049867	331.352069	5.232461
3.855999	345.039979	5.237466
4.188591	335.168419	5.242470
4.076457	341.357197	5.247475
4.001436	335.741029	5.252480
4.357689	342.117468	5.257485
3.891710	341.088418	5.262490
4.236819	345.492343	5.267494
3.931577	345.109401	5.272499
4.031111	347.966807	5.277504
4.276432	336.724783	5.282509
3.766818	343.961726	5.287514
4.206147	339.206421	5.292518
4.236288	339.494538	5.297523
4.268679	335.733512	5.302528
4.151072	341.585552	5.307533
3.840119	333.235666	5.312538
3.989180	332.006498	5.317542
3.904047	339.792196	5.322547
3.957044	337.411093	5.327552
4.003190	332.626767	5.332557
3.712347	337.594215	5.337562
4.335540	332.322423	5.342566
4.118252	334.831103	5.347571
4.118043	339.235572	5.352576
4.076593	335.169850	5.357581
4.378236	343.745382	5.362586
4.168166	340.113307	5.367590
4.186575	344.751894	5.372595
4.096456	344.751684	5.377600
4.495514	357.228438	5.382605
4.443995	369.377640	5.387610
4.364257	345.977984	5.392614
4.122141	348.709427	5.397619
4.120304	355.259229	5.402624
4.564492	364.557894	5.407629
4.533572	376.500432	5.412634
4.559029	364.068736	5.417638
4.227429	371.340349	5.422643
4.182289	375.103619	5.427648
4.286968	368.567294	5.432653
4.513975	372.291222	5.437658
4.774550	372.776408	5.442662
4.403986	375.799478	5.447667
4.673598	372.820285	5.452672
4.734235	373.247212	5.457677
4.453292	372.162261	5.462682
4.544179	370.542918	5.467686
4.318456	379.758540	5.472691
4.211076	367.558213	5.477696
4.734875	371.935122	5.482701
4.614252	374.045360	5.487706
4.711186	369.655379	5.492710
4.380724	368.171324	5.497715
4.241174	366.997838	5.502720
4.298823	369.074412	5.507725
4.171920	375.266635	5.512730
4.461272	375.298903	5.517734
4.114697	370.741808	5.522739
4.513576	382.848209	5.527744
4.247411	389.738000	5.532749
4.338633	394.322315	5.537754
4.770936	392.543028	5.542758
4.454315	390.862497	5.547763
4.459045	395.452846	5.552768
4.919343	396.005012	5.557773
4.461478	404.413495	5.562778
4.731741	393.416934	5.567782
4.927123	389.444789	5.572787
4.796133	392.880490	5.577792
4.610297	396.954979	5.582797
4.619064	396.387032	5.587802
5.092270	384.734270	5.592806
4.746699	395.912539	5.597811
4.852575	392.677077	5.602816
5.046449	389.071837	5.607821
4.724963	397.956604	5.612826
4.933348	395.697567	5.617830
4.636470	395.743830	5.622835
4.580587	394.689889	5.627840
5.001036	417.265283	5.632845
4.735169	421.144050	5.637850
5.291079	422.256415	5.642854
5.055081	422.109467	5.647859
5.010852	409.149356	5.652864
5.016652	401.892332	5.657869
5.078377	418.249015	5.662874
4.831602	406.943778	5.667878
4.866494	414.736279	5.672883
5.101851	414.758346	5.677888
5.416160	417.250448	5.682893
5.007189	422.211040	5.687898
5.343975	420.371789	5.692902
5.097908	413.106540	5.697907
5.180178	391.942866	5.702912
5.058686	394.090350	5.707917
4.999113	404.700493	5.712922
5.213550	408.931893	5.717926
5.217221	417.364798	5.722931
5.368920	407.665427	5.727936
5.058886	393.126436	5.732941
4.923614	405.924963	5.737946
5.241590	408.933877	5.742950
5.222827	420.673546	5.747955
5.194036	421.399253	5.752960
5.459155	410.847937	5.757965
5.211374	423.438367	5.762970
5.464061	417.020189	5.767974
5.244473	424.610530	5.772979
5.291870	424.962294	5.777984
5.218810	421.167599	5.782989
5.242947	425.118129	5.787994
5.403951	411.867887	5.792998
5.487216	421.798633	5.798003
5.210678	416.914185	5.803008
5.560251	415.837306	5.808013
5.056704	418.348210	5.813018
5.231692	415.872498	5.818022
5.207252	419.593673	5.823027
5.286192	422.651446	5.828032
5.487541	418.269421	5.833037
5.104730	427.380840	5.838042
5.634963	422.332802	5.843046
5.350200	423.519253	5.848051
4.871287	422.905764	5.853056
5.166021	419.259936	5.858061
5.362578	425.653184	5.863066
5.505413	432.900137	5.868070
5.245687	441.856006	5.873075
5.359269	452.834554	5.878080
5.846141	450.841190	5.883085
5.531858	459.997720	5.888090
5.868704	454.553666	5.893094
5.706267	449.381538	5.898099
5.666199	454.727829	5.903104
5.863734	454.207754	5.908109
5.704453	443.614999	5.913114
5.598747	421.844020	5.918118
5.381464	431.693508	5.923123
5.514712	447.074773	5.928128
5.634972	449.214005	5.933133
5.413027	454.940294	5.938138
5.935051	449.547277	5.943142
5.698404	448.145361	5.948147
5.877993	451.802762	5.953152
5.963867	453.944334	5.958157
5.917211	450.094938	5.963162
6.050113	443.946217	5.968166
5.942171	444.101304	5.973171
5.556221	435.914547	5.978176
5.830962	436.672678	5.983181
5.714860	453.026875	5.988186
6.074864	443.499011	5.993190
5.952372	451.315618	5.998195
5.784799	444.975899	6.003200
5.884663	441.581974	6.008205
5.579814	459.137058	6.013210
5.851008	456.001097	6.018214
6.025255	457.204884	6.023219
6.147080	452.818652	6.028224
5.920865	448.714230	6.033229
5.521092	438.457703	6.038234
5.765897	448.776720	6.043238
5.725244	450.854782	6.048243
5.781450	451.923402	6.053248
5.924987	445.961773	6.058253
5.978639	456.652463	6.063258
5.649509	454.743702	6.068262
5.523416	455.551631	6.073267
5.634911	454.032272	6.078272
5.914478	452.591842	6.083277
5.678935	461.343616	6.088282
5.712100	458.647273	6.093286
5.609219	456.887138	6.098291
5.707674	454.989271	6.103296
5.833365	452.415548	6.108301
5.660520	458.218366	6.113306
5.753891	456.032240	6.118310
5.972166	455.410654	6.123315
5.840153	452.083934	6.128320
5.833361	458.470808	6.133325
6.033362	465.400857	6.138330
6.081697	448.988924	6.143334
5.936193	468.021354	6.148339
5.718457	465.453189	6.153344
6.019728	453.502644	6.158349
5.941758	460.981736	6.163354
6.021859	452.055133	6.168358
5.869650	465.904976	6.173363
5.863497	457.580131	6.178368
5.880441	453.892282	6.183373
5.885493	454.159888	6.188378
6.138925	454.284933	6.193382
6.065508	459.980118	6.198387
6.134515	457.632655	6.203392
6.328478	455.812709	6.208397
5.840927	464.448541	6.213402
6.068952	465.354125	6.218406
5.800224	462.059317	6.223411
5.900256	460.968107	6.228416
6.005797	461.117247	6.233421
5.858219	463.475477	6.238426
5.773793	460.602451	6.243430
5.972422	456.506415	6.248435
5.922063	452.833657	6.253440
5.936912	440.494827	6.258445
5.506285	450.779660	6.263450
5.871585	452.082251	6.268454
6.018367	467.732834	6.273459
5.972971	457.819396	6.278464
6.047018	455.188510	6.283469
5.543400	449.814760	6.288474
5.753874	455.898262	6.293478
6.202164	458.667745	6.298483
5.598037	455.999970	6.303488
5.988470	458.855799	6.308493
5.701312	463.668554	6.313498
5.867910	454.409122	6.318502
5.823281	459.954692	6.323507
5.749197	460.587456	6.328512
5.900926	455.956898	6.333517
5.663608	456.530257	6.338522
5.933827	465.100207	6.343526
6.012416	460.700016	6.348531
5.978562	458.548770	6.353536
6.228777	459.074946	6.358541
5.311952	466.425948	6.363546
6.117701	454.959215	6.368550
5.808026	454.576609	6.373555
5.561722	463.010871	6.378560
5.989323	454.619136	6.383565
5.832660	465.947923	6.388570
6.148134	457.088905	6.393574
6.022962	459.697596	6.398579
5.835223	462.817890	6.403584
5.892027	460.742407	6.408589
5.517452	462.487402	6.413594
5.839693	454.880367	6.418598
5.897733	455.726479	6.423603
5.731296	461.090935	6.428608
6.116082	463.874092	6.433613
5.685369	472.370273	6.438618
5.818211	458.321681	6.443622
5.867884	463.534909	6.448627
5.970876	466.268625	6.453632
6.111492	463.134353	6.458637
5.486010	465.974686	6.463642
5.865219	465.061424	6.468646
6.052504	456.099310	6.473651
6.149411	464.856619	6.478656
5.879464	459.892919	6.483661
5.418622	460.663531	6.488666
5.616858	457.481239	6.493670
5.674796	463.276431	6.498675
5.771307	457.611686	6.503680
5.825381	460.310481	6.508685
5.764933	458.501680	6.513690
5.793629	460.021237	6.518694
5.820168	466.724850	6.523699
5.446823	465.649273	6.528704
5.764903	462.108501	6.533709
5.510357	470.567221	6.538714
5.628180	467.449156	6.543718
5.762646	470.117077	6.548723
5.767484	475.184401	6.553728
6.089133	490.207915	6.558733
5.955500	481.026599	6.563738
5.882636	478.212830	6.568742
5.991759	469.739238	6.573747
5.742322	468.219653	6.578752
6.211710	462.354432	6.583757
5.799910	463.928775	6.588762
5.641628	464.926745	6.593766
5.628603	465.096307	6.598771
5.452196	481.091693	6.603776
5.968158	481.367250	6.608781
5.761505	500.680990	6.613786
6.316496	487.848331	6.618790
5.914977	490.463518	6.623795
5.795961	475.756061	6.628800
6.264418	473.539593	6.633805
5.870251	472.048710	6.638810
5.756365	464.269583	6.643814
5.639721	472.176403	6.648819
5.826492	470.703976	6.653824
6.191256	470.903928	6.658829
6.110123	475.824063	6.663834
5.848143	465.500695	6.668838
6.102262	467.782147	6.673843
5.940574	454.762710	6.678848
5.915361	454.221503	6.683853
5.841862	460.042209	6.688858
5.859324	456.207848	6.693862
5.942376	470.295801	6.698867
5.997855	460.959845	6.703872
5.743893	457.985636	6.708877
5.812510	459.105877	6.713882
5.887624	467.323127	6.718886
5.775133	464.461260	6.723891
5.862553	462.342227	6.728896
5.733106	468.873148	6.733901
5.567319	466.858993	6.738906
5.757715	462.132242	6.743910
6.302073	463.812886	6.748915
5.847511	463.057818	6.753920
5.786799	457.492912	6.758925
5.902982	471.882440	6.763930
5.974559	455.733454	6.768934
6.136261	464.759071	6.773939
5.852864	467.070131	6.778944
6.010022	463.802285	6.783949
5.668358	472.894090	6.788954
5.648911	469.689429	6.793958
5.825910	465.444824	6.798963
5.482440	465.768367	6.803968
6.113613	461.199316	6.808973
5.456235	465.063989	6.813978
5.509184	470.426062	6.818982
5.837675	489.146971	6.823987
5.934213	494.308047	6.828992
6.497459	495.177857	6.833997
5.804248	475.345265	6.839002
5.633723	472.201142	6.844006
5.777227	470.443226	6.849011
5.809667	478.754575	6.854016
6.005037	490.464364	6.859021
6.046583	494.247251	6.864026
5.794644	473.505267	6.869030
5.778379	471.552195	6.874035
5.455213	470.516262	6.879040
6.264824	484.201721	6.884045
6.145856	482.205269	6.889050
6.023403	469.507893	6.894054
6.041313	465.635172	6.899059
5.852185	470.540825	6.904064
6.159216	457.854236	6.909069
5.669938	470.386419	6.914074
6.068941	465.371148	6.919078
5.920932	462.948914	6.924083
5.817058	454.383316	6.929088
6.101093	461.836407	6.934093
5.792458	474.579829	6.939098
6.167131	465.837892	6.944102
6.171372	471.169352	6.949107
5.789508	463.502287	6.954112
6.196350	461.633276	6.959117
5.878305	464.662467	6.964122
5.855404	460.618505	6.969126
6.317149	460.262083	6.974131
5.795628	473.703026	6.979136
6.005203	464.208741	6.984141
5.792834	462.458053	6.989146
6.139037	464.570923	6.994150
6.102129	451.706064	6.999155
5.471372	451.351169	7.004160
5.764596	450.633697	7.009165
5.702288	458.355684	7.014170
5.970920	457.502964	7.019174
6.077189	460.065832	7.024179
5.877457	467.294144	7.029184
6.024108	464.285368	7.034189
5.457076	454.953827	7.039194
5.921128	453.976393	7.044198
6.143076	454.821412	7.049203
5.972305	459.720076	7.054208
5.948094	440.081441	7.059213
5.785703	436.758176	7.064218
5.927608	436.145882	7.069222
6.231673	439.458836	7.074227
5.862238	439.808187	7.079232
5.882913	435.899889	7.084237
5.829037	435.000326	7.089242
6.112615	437.073242	7.094246
6.211804	433.103793	7.099251
5.597237	429.633005	7.104256
6.109561	425.833137	7.109261
6.178661	428.779269	7.114266
5.878465	430.654620	7.119270
5.836792	427.566328	7.124275
5.810345	424.420656	7.129280
5.917455	424.749508	7.134285
6.078897	430.972548	7.139290
6.017937	430.258472	7.144294
6.087601	428.834055	7.149299
5.791415	429.108326	7.154304
6.090784	434.101407	7.159309
5.759438	435.870223	7.164314
5.780428	438.518054	7.169318
5.928723	432.378037	7.174323
5.758487	431.671795	7.179328
5.873519	429.906955	7.184333
5.695483	433.986872	7.189338
5.675293	428.072885	7.194342
5.693249	427.327192	7.199347
5.872804	425.602384	7.204352
5.843854	431.362025	7.209357
5.337282	438.137328	7.214362
5.729342	435.970023	7.219366
5.577073	438.724888	7.224371
5.428962	436.139081	7.229376
5.847445	443.478136	7.234381
5.707690	459.233387	7.239386
6.228388	453.933139	7.244390
6.255177	452.908129	7.249395
6.056023	449.671858	7.254400
5.871919	439.933548	7.259405
5.997481	435.956574	7.264410
5.923638	431.749765	7.269414
5.842299	429.632040	7.274419
5.589622	437.176953	7.279424
5.706279	425.597015	7.284429
5.579833	432.693390	7.289434
5.904766	448.814312	7.294438
5.891969	444.164431	7.299443
5.397092	442.168464	7.304448
5.676974	451.438147	7.309453
5.776112	463.526165	7.314458
6.183948	460.470785	7.319462
6.041003	460.602462	7.324467
5.892771	468.426695	7.329472
5.972103	457.467624	7.334477
5.808761	471.246497	7.339482
5.994705	462.717957	7.344486
5.993038	466.453922	7.349491
5.759190	456.017366	7.354496
6.002045	447.875864	7.359501
5.941824	443.805526	7.364506
5.903886	445.285793	7.369510
5.705747	434.118908	7.374515
5.507429	444.000981	7.379520
6.105768	450.826581	7.384525
6.076760	458.271910	7.389530
5.884228	451.714907	7.394534
5.955606	443.219360	7.399539
5.986659	439.249155	7.404544
6.149498	420.982056	7.409549
5.609108	432.331538	7.414554
5.787332	430.705817	7.419558
6.021407	424.361562	7.424563
5.647786	436.486993	7.429568
5.650452	427.265379	7.434573
5.928086	434.508364	7.439578
6.097841	440.281085	7.444582
6.269793	434.095906	7.449587
5.880611	434.959240	7.454592
5.788962	433.440763	7.459597
5.687602	436.407822	7.464602
5.549289	435.277146	7.469606
5.800150	437.059472	7.474611
5.393376	429.421610	7.479616
6.125219	442.677675	7.484621
6.092594	461.038806	7.489626
5.871308	450.104260	7.494630
6.083837	440.609896	7.499635
5.708641	436.903117	7.504640
6.045208	426.448298	7.509645
5.795195	426.438847	7.514650
5.730293	427.224210	7.519654
5.792167	434.725323	7.524659
5.826959	450.979937	7.529664
5.911886	440.173087	7.534669
5.950479	439.800893	7.539674
5.944487	436.985531	7.544678
5.863085	431.128053	7.549683
5.722388	428.814136	7.554688
5.688897	442.093329	7.559693
6.002453	457.874354	7.564698
6.121076	452.585037	7.569702
6.270944	445.021942	7.574707
5.747489	440.939510	7.579712
5.870933	439.532827	7.584717
6.073875	437.531028	7.589722
5.495766	439.229604	7.594726
5.672774	433.054048	7.599731
5.890383	439.513476	7.604736
5.950743	440.359599	7.609741
5.884866	444.219463	7.614746
5.741314	433.447097	7.619750
5.721927	430.471347	7.624755
5.720132	450.701682	7.629760
5.949292	453.402465	7.634765
6.180193	464.333572	7.639770
6.016759	455.876703	7.644774
6.049140	436.151345	7.649779
5.542955	443.618060	7.654784
6.023873	431.469455	7.659789
5.934528	437.965700	7.664794
5.800605	438.811828	7.669798
5.933528	428.796654	7.674803
5.713501	436.092052	7.679808
5.676351	433.502277	7.684813
5.702707	432.812224	7.689818
6.091714	442.943962	7.694822
6.149667	437.848222	7.699827
5.941290	435.801656	7.704832
6.026754	434.090060	7.709837
5.832343	435.493029	7.714842
5.778610	439.810483	7.719846
6.015066	436.570755	7.724851
5.286832	435.288921	7.729856
5.607796	434.729661	7.734861
5.626819	453.462305	7.739866
5.842124	462.772486	7.744870
6.267279	458.085995	7.749875
5.903491	463.303158	7.754880
6.199919	455.813472	7.759885
5.779357	444.135795	7.764890
5.562778	439.815075	7.769894
5.968844	443.913716	7.774899
6.240960	450.567974	7.779904
6.337949	443.220447	7.784909
6.399728	438.082238	7.789914
6.390767	430.496115	7.794918
6.428288	437.501404	7.799923
6.109272	439.124713	7.804928
6.543152	426.652964	7.809933
5.839518	410.788290	7.814938
5.745947	409.623961	7.819942
5.715013	408.162528	7.824947
5.531722	402.308119	7.829952
5.885816	394.699785	7.834957
5.711792	408.683038	7.839962
5.834947	420.178384	7.844966
5.931473	435.266554	7.849971
5.805425	423.860404	7.854976
6.038929	432.765774	7.859981
5.683741	415.364936	7.864986
5.813399	429.153073	7.869990
6.380713	428.012905	7.874995
5.949800	417.633871	7.880000
5.811073	412.654773	7.885005
5.636662	411.563624	7.890010
5.782125	411.313253	7.895014
5.641081	409.204825	7.900019
6.065433	423.953150	7.905024
5.944254	407.727992	7.910029
5.805172	409.678882	7.915034
5.630763	413.698400	7.920038
5.927360	428.325011	7.925043
5.803038	435.400513	7.930048
5.978729	434.735855	7.935053
5.927250	443.948119	7.940058
5.768059	428.104769	7.945062
5.721786	435.181752	7.950067
5.812137	442.046275	7.955072
5.684277	436.583075	7.960077
6.112078	441.950556	7.965082
6.103021	443.139702	7.970086
5.895739	425.050908	7.975091
5.738002	425.543204	7.980096
6.088846	429.252559	7.985101
5.936808	411.521485	7.990106
5.735877	411.937262	7.995110
5.943837	403.611130	8.000115
5.544515	405.230298	8.005133
5.384904	419.694630	8.010150
5.977495	434.812900	8.015168
6.188749	440.164376	8.020186
5.987039	430.422808	8.025203
5.875751	439.255578	8.030221
6.044257	437.008224	8.035238
6.058533	431.889586	8.040256
5.680085	429.791460	8.045274
5.941067	423.876323	8.050291
5.779845	435.041587	8.055309
5.736493	430.205305	8.060326
5.800049	432.671620	8.065344
5.676556	432.579936	8.070362
6.031809	434.622781	8.075379
5.727569	444.740164	8.080397
5.939419	434.203986	8.085414
5.878096	436.831127	8.090432
5.806806	437.981293	8.095450
5.861596	435.240407	8.100467
5.707070	430.521543	8.105485
5.928836	426.001964	8.110502
5.945022	430.741497	8.115520
5.697689	436.250203	8.120538
6.292418	428.365576	8.125555
5.748094	438.810681	8.130573
6.181059	432.458628	8.135590
6.095494	438.022234	8.140608
5.682140	436.847533	8.145626
5.804671	436.034059	8.150643
5.929129	439.315423	8.155661
6.005717	443.077907	8.160678
6.286311	437.733685	8.165696
5.746800	441.842264	8.170714
6.041264	431.741390	8.175731
5.740987	438.404247	8.180749
6.241065	455.656001	8.185766
6.117772	453.347129	8.190784
5.848432	457.130287	8.195802
6.357586	454.253534	8.200819
6.200570	450.120465	8.205837
5.831445	436.764571	8.210854
6.100923	454.637929	8.215872
6.059726	457.057622	8.220890
6.056539	449.706213	8.225907
5.752578	470.878041	8.230925
5.969712	467.000705	8.235942
6.377668	462.835491	8.240960
5.950402	468.391718	8.245978
6.125880	465.781028	8.250995
5.886798	467.396152	8.256013
6.077325	469.400732	8.261030
5.990597	464.613155	8.266048
5.697592	476.835626	8.271066
6.155296	465.199348	8.276083
5.936623	468.089342	8.281101
5.908030	466.075788	8.286118
5.915965	466.739447	8.291136
5.718720	472.231800	8.296154
6.020443	469.623431	8.301171
6.401434	488.141894	8.306189
6.269971	477.490897	8.311206
6.257249	472.471394	8.316224
5.984122	472.748162	8.321242
6.360625	481.488372	8.326259
6.174899	481.641227	8.331277
6.028042	481.880946	8.336294
6.395462	485.575007	8.341312
6.161368	484.412348	8.346330
6.172866	472.983799	8.351347
6.300710	488.988468	8.356365
6.289412	488.505989	8.361382
6.258093	471.177488	8.366400
6.076750	477.759452	8.371418
6.471822	484.190068	8.376435
6.379829	473.988802	8.381453
6.339446	470.711939	8.386470
6.529790	466.618189	8.391488
6.110066	462.659711	8.396506
6.437585	460.498810	8.401523
6.487631	460.163248	8.406541
6.738241	467.414175	8.411558
6.493813	459.911187	8.416576
6.408165	472.295760	8.421594
6.638354	458.521536	8.426611
6.482855	465.159052	8.431629
6.562859	464.064453	8.436646
6.604831	460.659987	8.441664
6.458130	472.776739	8.446682
6.426972	467.955945	8.451699
6.356593	461.030193	8.456717
6.124064	459.410027	8.461734
6.541444	468.702474	8.466752
6.094970	468.611126	8.471770
6.394454	456.962473	8.476787
6.440039	465.936592	8.481805
6.574051	464.625584	8.486822
6.736191	454.808594	8.491840
6.081152	443.314272	8.496858
6.356447	445.042037	8.501875
6.391222	464.656306	8.506893
6.307925	465.189610	8.511910
6.414480	466.904181	8.516928
6.236264	478.632091	8.521946
6.097922	458.956936	8.526963
6.095107	464.749546	8.531981
5.986315	469.801497	8.536998
6.300761	464.492799	8.542016
6.396017	469.619615	8.547034
6.587920	466.034230	8.552051
6.517603	460.928410	8.557069
6.406020	466.700452	8.562087
6.393234	457.633829	8.567104
6.357773	470.171888	8.572122
6.505376	460.382694	8.577139
6.338856	469.372844	8.582157
6.482127	467.422555	8.587175
6.552976	467.447498	8.592192
6.313019	473.893507	8.597210
6.456692	473.247384	8.602227
6.362980	473.301544	8.607245
6.057047	466.854723	8.612263
6.430955	473.789195	8.617280
6.356664	486.501008	8.622298
6.607162	508.904008	8.627315
6.398042	504.971664	8.632333
6.767694	508.472462	8.637351
6.411843	499.232325	8.642368
6.354675	501.302727	8.647386
6.515405	493.621420	8.652403
6.614006	501.967928	8.657421
5.944913	503.159809	8.662439
6.493962	494.670948	8.667456
6.333656	503.810471	8.672474
6.361055	497.300763	8.677491
6.565072	500.545149	8.682509
6.293243	493.434646	8.687527
6.410924	493.912626	8.692544
6.372283	500.430618	8.697562
6.758194	490.135442	8.702579
6.403144	498.172648	8.707597
6.347904	508.798603	8.712615
6.826462	517.850848	8.717632
6.844566	524.147657	8.722650
6.711873	514.403268	8.727667
6.637540	507.092745	8.732685
6.565374	503.832161	8.737703
6.798355	504.956552	8.742720
6.639888	502.701525	8.747738
6.779906	503.448621	8.752755
6.715714	503.089262	8.757773
6.632723	506.666193	8.762791
7.050701	497.519949	8.767808
6.850970	500.720570	8.772826
6.586479	489.185359	8.777843
6.834996	490.361897	8.782861
6.622752	499.768660	8.787879
6.909990	495.835617	8.792896
6.687998	501.202757	8.797914
6.713828	495.794214	8.802931
6.755465	494.490627	8.807949
6.667700	494.779612	8.812967
6.683309	489.236356	8.817984
6.305412	498.096970	8.823002
6.418175	500.289221	8.828019
6.859140	511.467217	8.833037
6.945459	524.715221	8.838055
7.229503	515.421275	8.843072
6.528266	509.520961	8.848090
6.823956	502.666257	8.853107
6.978516	499.233494	8.858125
6.555359	507.488070	8.863143
6.735688	494.022246	8.868160
6.991996	514.000651	8.873178
6.674178	490.172211	8.878195
6.631722	502.150079	8.883213
6.762436	530.065064	8.888231
7.134630	525.891190	8.893248
7.086730	526.351908	8.898266
6.790775	516.261942	8.903283
6.837644	504.479900	8.908301
6.428040	508.459709	8.913319
6.686289	515.932212	8.918336
6.845084	526.804804	8.923354
6.939653	536.159406	8.928371
7.136592	526.538957	8.933389
6.743058	528.166672	8.938407
7.012530	526.285629	8.943424
6.948004	525.795035	8.948442
6.986506	526.372932	8.953459
7.232543	525.569512	8.958477
6.834103	526.022533	8.963495
7.258421	518.748518	8.968512
7.067105	510.153325	8.973530
6.903500	500.698886	8.978547
7.013311	494.930792	8.983565
6.527352	502.698951	8.988583
6.829353	508.916659	8.993600
6.928720	523.435440	8.998618
7.206721	517.877659	9.003635
7.271806	515.479124	9.008653
6.503855	516.295476	9.013671
6.550300	523.646767	9.018688
6.662762	531.395369	9.023706
6.920745	529.068820	9.028723
7.183427	519.304624	9.033741
6.965260	529.716448	9.038759
7.154710	526.023196	9.043776
7.060230	530.747229	9.048794
7.096876	528.717352	9.053811
7.077071	518.809002	9.058829
6.925366	529.261195	9.063847
6.822030	527.637935	9.068864
7.281938	519.679729	9.073882
7.137733	522.275533	9.078899
7.358965	528.451509	9.083917
7.100991	536.370895	9.088935
7.103631	521.783765	9.093952
7.292110	521.475866	9.098970
7.093336	524.818448	9.103987
7.389817	526.649597	9.109005
6.934283	528.167115	9.114023
7.242879	524.712383	9.119040
7.375340	527.664905	9.124058
7.063418	515.625951	9.129075
7.114023	504.558790	9.134093
6.864554	513.620177	9.139111
7.227901	517.111785	9.144128
7.190655	523.746279	9.149146
7.094344	534.114308	9.154163
7.393278	524.257891	9.159181
7.262046	525.051480	9.164199
7.488032	512.864995	9.169216
7.242827	509.725576	9.174234
6.659564	500.101276	9.179251
6.782685	502.220558	9.184269
7.111187	531.728267	9.189287
6.749057	532.957307	9.194304
7.059120	540.349593	9.199322
6.953398	539.153665	9.204339
7.297465	530.094242	9.209357
7.029029	539.200711	9.214375
7.130946	530.728591	9.219392
7.236045	530.504966	9.224410
7.140234	532.145975	9.229427
7.027465	537.164750	9.234445
7.104708	538.339930	9.239463
7.227069	536.829876	9.244480
7.108684	532.504180	9.249498
6.994113	553.004647	9.254515
7.665363	558.303417	9.259533
7.455698	559.656217	9.264551
7.466952	550.510367	9.269568
7.082878	541.628987	9.274586
7.255380	546.080091	9.279603
7.381458	542.763839	9.284621
6.984087	545.740521	9.289639
7.518668	557.265621	9.294656
7.613350	566.449566	9.299674
7.499551	562.188453	9.304691
7.466800	545.434870	9.309709
7.344655	535.647189	9.314727
6.829221	533.876632	9.319744
6.935901	551.662303	9.324762
7.294242	556.044057	9.329779
7.828685	559.171146	9.334797
7.614671	563.606540	9.339815
7.178510	573.709436	9.344832
7.635376	558.247308	9.349850
7.727460	571.368815	9.354867
7.717449	548.213872	9.359885
7.729412	531.617061	9.364903
7.298864	531.939975	9.369920
7.498250	526.581810	9.374938
7.522139	524.433582	9.379955
7.366371	530.202139	9.384973
7.239999	527.456789	9.389991
7.373371	521.377916	9.395008
6.965614	521.282125	9.400026
7.173911	542.591848	9.405043
7.561128	538.292263	9.410061
7.518506	551.159110	9.415079
7.647390	561.125325	9.420096
7.721177	550.003903	9.425114
7.470003	555.270586	9.430131
7.883718	548.761646	9.435149
7.691897	541.887658	9.440167
7.390654	528.649766	9.445184
7.507142	532.850121	9.450202
7.352867	546.558622	9.455219
7.626816	554.793058	9.460237
7.629251	554.546278	9.465255
7.767493	554.159694	9.470272
7.556611	539.822063	9.475290
7.140230	535.257543	9.480307
7.584091	547.789518	9.485325
7.685057	555.741990	9.490343
7.816493	549.409114	9.495360
8.000512	549.162775	9.500378
7.582296	543.551386	9.505395
7.420923	524.977128	9.510413
7.410007	537.624358	9.515431
7.385648	549.281178	9.520448
7.577799	556.160751	9.525466
7.446434	562.255767	9.530483
7.600166	558.484964	9.535501
7.559813	558.987343	9.540519
7.237163	561.926263	9.545536
7.787998	553.287085	9.550554
7.454042	557.097107	9.555571
7.511229	558.375012	9.560589
7.562725	564.449591	9.565607
7.357024	562.347643	9.570624
7.399160	559.332275	9.575642
7.244980	561.738806	9.580659
7.746071	578.417143	9.585677
7.933757	589.194253	9.590695
7.797721	584.831508	9.595712
7.805826	582.050693	9.600730
8.247653	587.463836	9.605747
7.932548	576.417617	9.610765
7.888086	556.047509	9.615783
8.008191	558.912325	9.620800
7.931675	554.909195	9.625818
7.683702	561.382550	9.630835
7.645115	549.644741	9.635853
8.000420	559.585469	9.640871
7.673646	555.700742	9.645888
7.494889	554.219487	9.650906
7.525367	560.577643	9.655923
7.755161	557.288108	9.660941
7.780929	562.813245	9.665959
7.976167	582.868579	9.670976
7.874280	571.398895	9.675994
7.600648	570.842144	9.681011
8.077426	581.958359	9.686029
8.081257	574.494910	9.691047
7.761148	570.713400	9.696064
7.821969	561.383167	9.701082
7.833615	573.959766	9.706099
7.728934	591.907443	9.711117
8.001516	584.680964	9.716135
7.980178	587.295800	9.721152
8.272300	588.400562	9.726170
7.893063	579.839794	9.731187
7.934509	565.435751	9.736205
7.940122	558.140113	9.741223
7.643255	557.081536	9.746240
8.061211	566.781793	9.751258
7.937089	584.219330	9.756275
8.030392	584.973378	9.761293
8.172624	581.730422	9.766311
7.915667	573.759997	9.771328
8.107545	563.519933	9.776346
8.142543	562.074142	9.781363
8.137389	554.196471	9.786381
8.176848	553.642400	9.791399
7.758478	565.480019	9.796416
7.764645	558.621267	9.801434
7.769688	568.449147	9.806451
7.974294	588.658045	9.811469
8.281456	586.740047	9.816487
8.330097	590.128480	9.821504
8.069615	570.601943	9.826522
7.989400	566.145320	9.831539
7.905539	563.070112	9.836557
8.083670	576.209262	9.841575
8.218489	588.023598	9.846592
8.269583	584.505595	9.851610
8.037278	564.689576	9.856627
7.765725	574.689827	9.861645
8.389419	585.735460	9.866663
7.951360	595.523352	9.871680
8.313338	587.384294	9.876698
8.269331	585.452601	9.881715
7.974242	593.174829	9.886733
8.492530	589.859168	9.891751
7.884015	576.406582	9.896768
8.357881	568.663348	9.901786
8.334332	579.092187	9.906803
8.397600	572.113548	9.911821
8.224091	566.824597	9.916839
8.011377	562.275947	9.921856
7.835578	556.948798	9.926874
8.169535	567.992007	9.931891
8.248203	574.981122	9.936909
8.789505	579.835111	9.941927
8.218868	573.069897	9.946944
8.289988	558.656812	9.951962
8.053352	564.530695	9.956979
8.060814	564.955083	9.961997
8.321127	565.159858	9.967015
8.192161	584.196316	9.972032
8.183443	586.819101	9.977050
8.318032	589.100068	9.982067
8.072137	588.916651	9.987085
8.481878	587.793621	9.992103
8.400522	591.760038	9.997120
8.422915	578.489180	10.002138
8.546444	586.368055	10.007155
8.249293	586.694272	10.012173
8.544597	573.414642	10.017191
8.280617	575.127791	10.022208
8.506838	580.759890	10.027226
8.207655	570.456067	10.032243
8.149153	582.516176	10.037261
8.567315	579.154502	10.042279
8.539707	584.257412	10.047296
8.358025	575.409029	10.052314
8.289536	571.039630	10.057331
8.101878	577.943329	10.062349
8.697676	573.233434	10.067367
8.423822	581.937703	10.072384
8.215308	574.531067	10.077402
8.462639	581.334196	10.082419
8.393679	588.199545	10.087437
8.621510	580.232890	10.092455
8.834849	584.980963	10.097472
8.373576	586.262838	10.102490
8.878466	579.974008	10.107507
8.415572	573.829492	10.112525
8.290372	556.555022	10.117543
8.493584	563.255023	10.122560
8.464710	577.926184	10.127578
8.593058	573.722404	10.132595
8.464624	582.070332	10.137613
8.605517	583.089120	10.142631
8.551542	580.001086	10.147648
8.474992	579.874858	10.152666
8.459010	579.475626	10.157683
8.465225	587.846926	10.162701
8.584658	581.528229	10.167719
8.326966	586.786161	10.172736
8.418740	581.886711	10.177754
8.091056	585.119166	10.182771
8.256083	587.826560	10.187789
8.736029	575.974128	10.192807
8.258281	583.408903	10.197824
8.241697	584.559075	10.202842
8.712389	588.004580	10.207859
8.454998	582.283874	10.212877
8.470939	587.077035	10.217895
8.647405	602.102773	10.222912
8.888677	601.509770	10.227930
8.603133	586.161299	10.232947
8.533371	599.660590	10.237965
8.688315	609.675470	10.242983
8.954410	610.685141	10.248000
8.667843	604.218914	10.253018
8.848306	597.567094	10.258035
8.481605	593.600589	10.263053
8.858162	603.863002	10.268071
8.281855	601.863162	10.273088
8.747010	605.726883	10.278106
9.148161	616.982803	10.283123
8.654600	617.131323	10.288141
9.113661	615.883005	10.293159
8.759682	599.017213	10.298176
8.572941	596.239921	10.303194
9.272809	598.037941	10.308211
8.714035	601.989132	10.313229
8.640781	585.392203	10.318247
8.553987	593.453536	10.323264
8.779232	610.128967	10.328282
8.949023	616.459551	10.333299
8.786518	622.232406	10.338317
9.146067	615.225748	10.343335
8.555321	614.697099	10.348352
8.767014	615.881515	10.353370
9.278064	624.172389	10.358387
8.987567	608.358014	10.363405
9.060586	597.763224	10.368423
8.815906	592.868504	10.373440
8.534015	587.288655	10.378458
9.064324	603.699602	10.383475
8.970672	612.587617	10.388493
8.894516	613.138444	10.393511
9.121583	606.332062	10.398528
9.224396	603.197984	10.403546
9.075738	587.352860	10.408563
8.828234	592.476241	10.413581
8.916012	580.880268	10.418599
8.386964	584.744844	10.423616
8.628743	601.873403	10.428634
8.835001	608.740822	10.433651
8.874754	617.945113	10.438669
8.831176	619.826285	10.443687
9.303412	616.788698	10.448704
9.169104	630.847881	10.453722
9.350592	622.643225	10.458739
9.014900	621.427698	10.463757
9.199106	620.899653	10.468775
9.133263	618.578487	10.473792
9.173749	619.657011	10.478810
9.115506	618.572695	10.483827
9.191146	631.424159	10.488845
9.110958	618.637349	10.493863
9.206611	615.512130	10.498880
8.850004	615.699778	10.503898
9.243946	614.924418	10.508915
8.723352	622.238756	10.513933
8.977783	621.154039	10.518951
9.259671	622.463831	10.523968
9.240636	631.473153	10.528986
9.307060	622.263995	10.534003
9.264670	634.460050	10.539021
8.839209	623.243108	10.544039
9.167149	626.509517	10.549056
8.847185	634.937611	10.554074
9.205750	616.669837	10.559091
9.126396	629.080066	10.564109
9.159986	623.073775	10.569127
9.368661	620.222341	10.574144
9.017857	621.180828	10.579162
9.032500	616.144741	10.584179
9.042726	620.989052	10.589197
9.032862	624.073421	10.594215
8.907125	614.943722	10.599232
8.735132	635.730757	10.604250
9.173108	639.012016	10.609267
9.104516	648.825961	10.614285
8.872414	647.509425	10.619303
9.501199	649.890642	10.624320
9.143649	654.055557	10.629338
9.326838	656.663701	10.634355
9.438312	650.609072	10.639373
9.395305	656.408410	10.644391
9.586313	655.458791	10.649408
9.283505	650.007769	10.654426
9.401998	645.751472	10.659443
9.157853	651.522700	10.664461
9.353257	652.201778	10.669479
9.479698	649.614137	10.674496
9.088651	652.565778	10.679514
9.562645	651.648822	10.684531
9.547434	647.212315	10.689549
9.328140	651.036245	10.694567
9.506353	646.838165	10.699584
9.181783	645.029887	10.704602
9.638249	647.396334	10.709619
9.158657	648.695419	10.714637
9.626578	652.834661	10.719655
9.543480	645.094252	10.724672
9.540350	649.452429	10.729690
9.700962	640.997693	10.734707
9.517334	649.762645	10.739725
9.516384	653.368148	10.744743
9.727526	647.737146	10.749760
9.528761	653.293394	10.754778
9.358180	642.610180	10.759795
9.292963	653.048331	10.764813
9.574474	657.799113	10.769831
9.544652	646.170205	10.774848
9.622406	655.500894	10.779866
9.538471	643.290435	10.784883
9.721977	653.070511	10.789901
9.475267	654.757385	10.794919
9.610343	655.026400	10.799936
9.313450	658.465963	10.804954
9.614113	653.007918	10.809971
9.705994	650.818101	10.814989
9.402485	657.905378	10.820007
9.735133	649.895743	10.825024
9.448998	656.481355	10.830042
9.537639	656.330528	10.835059
9.709593	651.095359	10.840077
9.531098	651.445431	10.845095
9.616885	648.604302	10.850112
9.713440	669.618550	10.855130
9.883347	664.615591	10.860147
9.840724	654.847341	10.865165
9.716477	647.923536	10.870183
9.681731	655.232039	10.875200
9.735774	656.173880	10.880218
9.872655	660.404158	10.885235
9.671930	655.221646	10.890253
9.772229	651.433685	10.895271
9.787357	650.764355	10.900288
10.244440	664.631946	10.905306
9.856701	660.657885	10.910323
9.804511	650.400308	10.915341
9.744261	653.312919	10.920359
9.749512	655.493077	10.925376
9.392278	655.672365	10.930394
10.056737	670.636259	10.935411
10.033072	671.676003	10.940429
9.926500	673.996325	10.945447
9.753699	656.154859	10.950464
9.826460	664.442352	10.955482
9.664729	676.055483	10.960499
9.814378	674.965870	10.965517
9.850003	686.280204	10.970535
9.908548	685.820599	10.975552
9.696601	683.932254	10.980570
10.084457	678.035379	10.985587
9.925323	675.510375	10.990605
9.965983	686.208559	10.995623
10.071301	670.353969	11.000640
10.109727	679.336483	11.005658
9.885934	683.919780	11.010675
10.131983	686.929307	11.015693
10.060716	690.275219	11.020711
10.246692	673.677787	11.025728
9.911538	681.846233	11.030746
10.047343	676.227302	11.035763
10.280578	676.017887	11.040781
9.811412	680.964630	11.045799
10.303880	690.954183	11.050816
9.957350	682.881809	11.055834
9.761697	678.304710	11.060851
9.963271	677.924565	11.065869
9.782703	679.821736	11.070887
9.983311	676.760420	11.075904
9.794977	681.816556	11.080922
9.874491	688.798693	11.085939
10.199374	675.339876	11.090957
9.844916	684.062667	11.095975
10.471882	676.134589	11.100992
10.227102	674.576858	11.106010
10.093315	690.076864	11.111027
9.963569	677.137395	11.116045
9.882684	679.115690	11.121063
10.106808	678.681814	11.126080
9.953459	689.390473	11.131098
10.010820	701.883037	11.136115
10.570010	700.683877	11.141133
10.529072	705.579008	11.146151
10.238694	694.044387	11.151168
10.017020	680.432384	11.156186
9.986635	688.784604	11.161203
10.328593	694.088346	11.166221
10.292849	700.995879	11.171239
10.397995	707.081708	11.176256
10.471353	708.088853	11.181274
10.468099	705.303401	11.186291
10.664535	687.204312	11.191309
10.143541	682.683841	11.196327
10.258736	677.369485	11.201344
10.498400	687.185556	11.206362
10.190467	675.787312	11.211379
10.486683	672.927081	11.216397
10.396111	680.016508	11.221415
10.191299	669.230682	11.226432
10.273343	691.189823	11.231450
10.542750	699.299899	11.236467
10.866750	698.975461	11.241485
10.399737	689.180226	11.246503
10.342492	680.206460	11.251520
10.248155	683.755785	11.256538
10.630101	682.669042	11.261555
10.447605	680.153811	11.266573
10.418175	677.812828	11.271591
10.268099	676.549238	11.276608
10.318886	691.032523	11.281626
10.421940	705.707153	11.286643
10.636241	704.536759	11.291661
10.404283	706.185764	11.296679
10.218990	704.083173	11.301696
10.464940	710.113012	11.306714
10.327960	712.278543	11.311731
10.420514	702.374107	11.316749
10.333864	710.853759	11.321767
10.340801	697.727476	11.326784
10.486094	707.064728	11.331802
10.665308	713.785500	11.336819
10.975242	705.443790	11.341837
10.482054	712.671549	11.346855
10.634287	706.712112	11.351872
10.879039	710.094670	11.356890
10.765714	705.111828	11.361907
10.871102	695.209996	11.366925
10.582113	702.930284	11.371943
10.868688	697.461566	11.376960
10.799669	701.863737	11.381978
10.499139	707.622277	11.386995
10.752003	705.089672	11.392013
10.463852	708.033733	11.397031
10.657355	704.580698	11.402048
10.739319	701.476429	11.407066
10.688690	705.431883	11.412083
10.430875	698.437658	11.417101
10.750744	711.068639	11.422119
11.048749	700.397157	11.427136
11.038398	702.305905	11.432154
10.885758	712.577087	11.437171
11.070707	703.276606	11.442189
10.525506	705.144400	11.447207
10.545893	700.650412	11.452224
11.235239	701.187468	11.457242
10.948286	705.502901	11.462259
10.772917	702.389278	11.467277
10.397931	697.261983	11.472295
10.589312	703.718940	11.477312
10.713445	704.310222	11.482330
10.377467	701.291694	11.487347
10.793026	714.315470	11.492365
11.264403	732.353736	11.497383
11.195630	731.919149	11.502400
11.116155	710.398994	11.507418
11.020792	712.632039	11.512435
11.039716	697.603096	11.517453
10.885228	701.109239	11.522471
10.925143	700.185031	11.527488
10.963325	691.684009	11.532506
10.969402	700.582133	11.537523
10.815608	693.791539	11.542541
11.321949	720.067598	11.547559
10.982580	710.706304	11.552576
10.748172	709.692095	11.557594
11.153143	718.993441	11.562611
11.437711	718.480662	11.567629
11.208130	706.644249	11.572647
11.165702	699.449801	11.577664
11.238492	691.754417	11.582682
11.076929	706.298861	11.587699
11.048216	696.176335	11.592717
11.025293	703.106154	11.597735
10.946502	707.968579	11.602752
11.217732	698.014482	11.607770
10.852138	695.551613	11.612787
11.080841	707.311520	11.617805
11.140700	719.526929	11.622823
11.133430	735.578045	11.627840
11.489749	737.616227	11.632858
11.219638	733.947059	11.637875
11.150512	726.396411	11.642893
11.257345	724.825724	11.647911
11.158033	726.665747	11.652928
11.863345	718.956944	11.657946
11.347685	715.593779	11.662963
11.594521	698.605556	11.667981
10.949721	693.566639	11.672999
10.830397	690.340595	11.678016
11.351001	713.496754	11.683034
11.164722	715.755090	11.688051
11.356018	722.661649	11.693069
11.253272	724.922688	11.698087
11.247424	734.992816	11.703104
11.353205	725.451115	11.708122
11.065114	721.608166	11.713139
11.230985	723.359791	11.718157
11.449656	723.221682	11.723175
11.452967	733.760344	11.728192
11.644047	721.866861	11.733210
11.402918	731.033483	11.738227
11.525030	723.210238	11.743245
11.175621	718.541272	11.748263
11.298615	724.364718	11.753280
11.426857	728.614555	11.758298
11.057074	724.846547	11.763315
11.525387	719.154825	11.768333
11.321092	727.666565	11.773351
11.070377	722.028949	11.778368
11.238653	719.499719	11.783386
10.982575	730.275808	11.788403
11.384207	745.911607	11.793421
11.519261	746.853817	11.798439
11.668822	751.319409	11.803456
11.400093	757.990760	11.808474
11.575777	756.670859	11.813491
11.780550	748.259537	11.818509
11.649840	751.444449	11.823527
11.593733	757.643215	11.828544
11.818981	750.091051	11.833562
11.667236	762.192329	11.838579
11.933316	754.303893	11.843597
12.003441	747.140389	11.848615
11.675371	739.786934	11.853632
11.800643	727.813403	11.858650
11.490803	729.822138	11.863667
11.792757	722.414363	11.868685
11.675459	720.900869	11.873703
11.661120	721.199745	11.878720
11.756521	713.359276	11.883738
11.738863	721.557053	11.888755
11.294638	725.052127	11.893773
11.923495	731.800413	11.898791
11.926905	738.684552	11.903808
11.806366	739.848209	11.908826
11.747623	733.143033	11.913843
11.808244	725.394926	11.918861
12.084755	744.742959	11.923879
11.978323	732.183419	11.928896
11.660644	723.114966	11.933914
11.689775	730.559375	11.938931
11.620772	735.573722	11.943949
11.710425	738.354447	11.948967
11.632797	749.743089	11.953984
12.010777	746.700024	11.959002
11.971630	751.431102	11.964019
12.183300	751.380761	11.969037
12.160807	752.239617	11.974055
11.985486	755.426800	11.979072
12.237268	747.524200	11.984090
11.909454	737.551169	11.989107
12.144538	735.499822	11.994125
12.017246	721.071807	11.999143
11.360245	730.691128	12.004160
11.975066	733.202223	12.009178
11.914643	751.359672	12.014195
12.036286	747.116211	12.019213
11.860766	745.505274	12.024231
11.760975	751.259329	12.029248
12.049944	743.760786	12.034266
12.214213	746.348064	12.039283
11.967689	749.978901	12.044301
12.277588	749.026518	12.049319
12.031173	752.173900	12.054336
12.372330	751.364758	12.059354
12.369933	749.191719	12.064371
12.163749	751.958445	12.069389
12.120356	748.138746	12.074407
12.126496	756.941621	12.079424
11.981803	743.373899	12.084442
12.243871	758.462381	12.089459
12.287176	756.547113	12.094477
12.482094	745.215543	12.099495
12.476398	757.605213	12.104512
12.404932	747.542092	12.109530
11.961889	738.085357	12.114547
12.133343	743.812602	12.119565
11.882348	738.596262	12.124583
11.841747	746.168361	12.129600
11.873028	738.877835	12.134618
12.234479	750.041418	12.139635
12.086985	741.354985	12.144653
12.294958	736.066189	12.149671
11.761550	752.259559	12.154688
11.758112	743.694538	12.159706
12.106996	770.072342	12.164723
12.167391	768.405016	12.169741
12.640189	768.355527	12.174759
12.416836	771.629008	12.179776
12.570412	772.246124	12.184794
12.490075	772.434677	12.189811
12.186171	777.243854	12.194829
12.283805	773.351979	12.199847
12.305211	773.690211	12.204864
12.342912	772.933678	12.209882
12.447974	775.003630	12.214899
12.308102	784.736555	12.219917
12.517381	777.151197	12.224935
12.525857	779.865454	12.229952
12.464879	775.908117	12.234970
12.593542	772.824839	12.239987
12.629328	779.432783	12.245005
12.703573	777.185242	12.250023
12.504200	773.137048	12.255040
13.060643	772.287138	12.260058
12.917671	778.426678	12.265075
12.243628	776.241631	12.270093
12.273693	771.431470	12.275111
12.573138	779.624799	12.280128
12.419754	770.935782	12.285146
12.873649	781.036499	12.290163
12.955456	774.983192	12.295181
12.890162	779.159190	12.300199
12.695712	774.666505	12.305216
12.941460	773.038167	12.310234
12.880616	771.109436	12.315251
12.640785	777.352018	12.320269
12.791914	770.836076	12.325287
12.842320	775.376752	12.330304
13.079047	769.563920	12.335322
12.961092	768.087142	12.340339
12.938285	771.014046	12.345357
13.189366	763.538696	12.350375
13.101589	753.957772	12.355392
12.977915	746.161043	12.360410
12.797788	740.689674	12.365427
12.356571	739.305007	12.370445
12.811949	742.057454	12.375463
12.717822	745.923275	12.380480
12.865338	756.997492	12.385498
13.020069	766.704456	12.390515
12.728357	780.456393	12.395533
12.924312	767.555036	12.400551
12.596302	774.773582	12.405568
12.750651	774.218588	12.410586
12.946679	773.320490	12.415603
12.735663	777.987128	12.420621
12.788435	765.553553	12.425639
12.805218	778.635148	12.430656
13.009273	772.588762	12.435674
13.014225	760.876455	12.440691
12.646289	775.983848	12.445709
12.763497	769.534544	12.450727
12.755848	779.784124	12.455744
12.811064	776.081153	12.460762
12.880657	776.736190	12.465779
12.934640	785.422111	12.470797
13.492360	790.929122	12.475815
13.303179	788.653550	12.480832
13.487979	780.537628	12.485850
13.437941	767.018774	12.490867
13.177212	768.259581	12.495885
13.379080	754.688789	12.500903
13.262972	762.845808	12.505920
13.213636	771.218926	12.510938
13.640100	760.078912	12.515955
13.277802	763.773015	12.520973
13.532688	759.777157	12.525991
13.377012	759.023514	12.531008
13.334335	765.594447	12.536026
13.735298	760.573669	12.541043
13.416579	764.871151	12.546061
13.061873	740.166790	12.551079
12.957259	748.764391	12.556096
12.989101	751.144478	12.561114
13.132585	757.488531	12.566131
13.398892	769.345402	12.571149
13.363382	770.478054	12.576167
13.529836	762.422262	12.581184
13.208690	771.036048	12.586202
13.696046	769.018510	12.591219
13.334210	766.273921	12.596237
13.400419	764.406824	12.601255
13.397707	769.087783	12.606272
13.396957	768.246284	12.611290
13.903219	767.553888	12.616307
13.460982	772.172202	12.621325
13.639623	763.825038	12.626343
13.687962	764.165896	12.631360
13.297718	765.567905	12.636378
13.463447	762.756429	12.641395
13.169120	769.311951	12.646413
13.584391	761.102367	12.651431
13.478427	769.513207	12.656448
13.322523	764.959813	12.661466
13.249797	760.948523	12.666483
13.056011	772.027300	12.671501
13.456376	760.896725	12.676519
13.400823	762.109856	12.681536
13.024803	767.785648	12.686554
13.387228	772.056952	12.691571
13.459838	790.777819	12.696589
13.492994	787.661537	12.701607
13.982518	794.476228	12.706624
13.399839	797.959601	12.711642
13.859284	792.322468	12.716659
13.771631	795.624662	12.721677
13.685967	793.045349	12.726695
13.723924	798.594338	12.731712
13.460500	794.990973	12.736730
13.615638	790.371501	12.741747
13.553156	795.389513	12.746765
13.915399	786.227331	12.751783
13.928042	791.874598	12.756800
13.693105	803.450737	12.761818
14.069632	791.458779	12.766835
13.853848	794.738098	12.771853
13.717253	788.027681	12.776871
14.043722	792.899006	12.781888
13.606863	801.803215	12.786906
13.845240	789.027485	12.791923
13.871694	794.472084	12.796941
13.898848	794.072396	12.801959
14.139400	794.579840	12.806976
13.719484	794.072696	12.811994
13.771875	793.693631	12.817011
13.682533	797.961801	12.822029
13.424894	794.837374	12.827047
13.859608	807.224626	12.832064
13.793398	824.584343	12.837082
14.491187	813.623366	12.842099
14.279726	819.917563	12.847117
14.385403	808.305071	12.852135
14.611625	793.223994	12.857152
14.317570	786.612087	12.862170
14.474816	779.758140	12.867187
14.259983	781.596433	12.872205
14.124657	782.207848	12.877223
14.510241	779.767815	12.882240
13.914794	781.232937	12.887258
14.421066	784.990688	12.892275
14.369020	785.353286	12.897293
14.080677	779.970685	12.902311
14.451116	782.943098	12.907328
14.124269	789.988633	12.912346
14.198887	783.989659	12.917363
14.124770	781.447410	12.922381
13.991046	791.428914	12.927399
14.392188	782.312653	12.932416
14.059553	793.664817	12.937434
14.305076	789.192969	12.942451
14.229755	789.751143	12.947469
14.147260	790.019970	12.952487
14.271280	792.378895	12.957504
14.002427	797.956641	12.962522
14.373489	788.506793	12.967539
14.417908	788.092042	12.972557
14.174687	779.699771	12.977575
14.609386	782.228890	12.982592
14.153134	785.763368	12.987610
14.283425	790.098705	12.992627
14.340896	791.905688	12.997645
14.322033	794.278037	13.002663
14.174541	783.354300	13.007680
14.155431	809.692325	13.012698
14.468381	817.195285	13.017715
14.812806	816.223009	13.022733
14.639203	829.876302	13.027751
14.570686	822.356607	13.032768
14.612698	819.850631	13.037786
14.733601	815.455707	13.042803
14.877663	814.867771	13.047821
14.811006	791.776959	13.052839
14.809584	790.359224	13.057856
14.325654	790.556342	13.062874
14.717250	790.805323	13.067891
14.603734	786.744878	13.072909
14.404554	789.097087	13.077927
14.597391	783.152943	13.082944
14.695965	801.751420	13.087962
14.835609	811.045973	13.092979
14.588756	802.416114	13.097997
14.737264	810.077002	13.103015
14.910234	810.642485	13.108032
14.632467	797.524287	13.113050
14.861409	801.596848	13.118067
14.883699	810.798634	13.123085
14.676300	811.574338	13.128103
14.893860	803.880516	13.133120
14.243042	807.940497	13.138138
14.809203	812.779619	13.143155
14.763788	822.861081	13.148173
14.645179	819.185702	13.153191
14.958956	812.045992	13.158208
14.641146	823.890185	13.163226
14.909166	816.257682	13.168243
14.959069	823.156206	13.173261
14.690160	822.440206	13.178279
14.962349	816.461257	13.183296
14.870950	821.931679	13.188314
14.658399	821.268549	13.193331
14.775383	817.391963	13.198349
14.402133	821.098128	13.203367
15.121326	819.795305	13.208384
14.967275	834.748446	13.213402
15.238014	839.257380	13.218419
15.449206	833.241283	13.223437
15.121523	828.480108	13.228455
15.111538	820.588929	13.233472
15.129797	821.552453	13.238490
15.092782	812.849654	13.243507
15.542709	817.177344	13.248525
15.167248	827.100873	13.253543
15.427766	813.301432	13.258560
15.237072	814.908579	13.263578
14.773872	826.098932	13.268595
14.880563	818.050646	13.273613
15.051862	826.569140	13.278631
15.363187	821.869074	13.283648
15.168555	823.705602	13.288666
15.274878	817.491533	13.293683
14.923565	816.014417	13.298701
15.422290	838.543319	13.303719
15.427290	831.539765	13.308736
15.381229	843.238586	13.313754
15.522219	839.017092	13.318771
15.364984	821.812194	13.323789
15.364432	832.466518	13.328807
15.442921	830.165513	13.333824
15.419578	837.093886	13.338842
15.300796	829.853363	13.343859
15.737278	829.685485	13.348877
15.328905	829.218157	13.353895
15.518307	824.972509	13.358912
15.570780	818.413832	13.363930
15.415463	820.618633	13.368947
15.640573	813.601866	13.373965
15.457621	818.463465	13.378983
15.609590	815.780235	13.384000
15.459699	810.401467	13.389018
15.353132	809.203492	13.394035
15.727135	823.357017	13.399053
15.419012	832.637149	13.404071
15.729061	821.902568	13.409088
15.613981	828.501265	13.414106
15.417295	831.534922	13.419123
15.800079	833.660463	13.424141
15.702312	829.650151	13.429159
15.797529	823.366270	13.434176
15.538385	837.503001	13.439194
15.853391	834.560500	13.444211
15.898854	839.897248	13.449229
15.843479	843.708254	13.454247
16.169657	824.477735	13.459264
15.729701	816.387692	13.464282
15.671271	822.277042	13.469299
15.545229	806.907057	13.474317
15.555664	821.957352	13.479335
15.778972	824.684072	13.484352
15.371890	828.317499	13.489370
15.807106	830.068235	13.494387
16.054988	824.895234	13.499405
15.351692	834.813215	13.504423
15.889527	829.969740	13.509440
15.724427	837.432584	13.514458
15.874031	834.506448	13.519475
15.553597	828.644129	13.524493
15.786839	833.218323	13.529511
15.916961	826.015321	13.534528
15.941479	831.523636	13.539546
15.967507	834.743238	13.544563
15.964225	829.767723	13.549581
15.787924	839.536635	13.554599
15.936667	844.611019	13.559616
16.071907	858.666718	13.564634
15.926482	854.810347	13.569651
16.253909	853.136194	13.574669
16.139697	869.895280	13.579687
16.603267	861.208771	13.584704
16.068169	852.843532	13.589722
16.081387	841.997074	13.594739
16.375205	841.828411	13.599757
15.857420	843.578301	13.604775
16.023952	845.929801	13.609792
16.131034	855.144342	13.614810
16.231513	862.249852	13.619827
16.564363	854.910123	13.624845
16.223083	863.095425	13.629863
16.315331	857.164366	13.634880
16.249316	865.620215	13.639898
16.494228	864.947077	13.644915
16.861909	854.251354	13.649933
16.135405	849.273942	13.654951
16.303565	845.334153	13.659968
16.722207	854.346325	13.664986
16.044613	849.866300	13.670003
16.359641	852.631772	13.675021
16.571170	858.542179	13.680039
16.400534	857.494960	13.685056
16.597641	856.243154	13.690074
16.351874	859.993963	13.695091
16.637186	849.758317	13.700109
16.580232	854.686460	13.705127
16.275599	862.183838	13.710144
16.412528	856.783542	13.715162
16.124475	853.825548	13.720179
16.802306	851.437501	13.725197
16.423964	857.113316	13.730215
16.342116	856.081708	13.735232
16.544535	855.071924	13.740250
15.987054	859.897132	13.745267
16.629411	848.769335	13.750285
16.320980	857.875526	13.755303
16.545815	844.581153	13.760320
16.306045	856.780147	13.765338
16.484845	874.977653	13.770355
17.009306	880.200848	13.775373
16.801390	878.568885	13.780391
16.943238	870.815916	13.785408
16.986745	879.435518	13.790426
16.706820	871.494528	13.795443
16.803373	864.461626	13.800461
16.857058	863.398521	13.805479
16.835660	863.553300	13.810496
17.094656	857.484399	13.815514
16.937221	853.012331	13.820531
17.287038	846.429601	13.825549
17.001885	846.089893	13.830567
17.031345	843.153731	13.835584
16.785431	834.691406	13.840602
16.778126	850.795006	13.845619
16.599123	834.050369	13.850637
16.652834	845.381902	13.855655
16.821730	857.542752	13.860672
17.063138	862.817930	13.865690
16.962176	866.516418	13.870707
17.206945	870.524175	13.875725
17.048188	873.157878	13.880743
17.088979	872.502793	13.885760
17.382928	872.138055	13.890778
17.239071	874.511429	13.895795
17.299437	867.790802	13.900813
17.270143	844.838205	13.905831
17.051088	856.893225	13.910848
17.244246	845.367395	13.915866
16.901697	849.734984	13.920883
16.998313	858.228857	13.925901
17.481568	865.949297	13.930919
17.241873	873.568598	13.935936
17.484959	873.752020	13.940954
17.107381	863.601723	13.945971
17.354163	861.691723	13.950989
17.323980	869.418054	13.956007
17.320787	866.538866	13.961024
17.778628	863.029428	13.966042
17.505816	849.090720	13.971059
17.291627	846.759834	13.976077
17.295238	850.468166	13.981095
17.202189	841.858090	13.986112
17.728475	845.276733	13.991130
17.310244	850.490671	13.996147
17.386235	844.644588	14.001165
17.061572	854.431777	14.006183
17.334403	863.746431	14.011200
17.925803	868.936492	14.016218
17.467700	875.899080	14.021235
17.645260	867.283943	14.026253
17.802820	863.782890	14.031271
17.488006	869.804866	14.036288
17.335657	869.742758	14.041306
17.510606	874.965168	14.046323
17.391724	867.555360	14.051341
17.437621	869.366631	14.056359
17.287687	865.325580	14.061376
17.445683	855.106681	14.066394
17.521113	867.645203	14.071411
17.611162	858.672532	14.076429
17.443866	861.490315	14.081447
17.502381	861.398409	14.086464
18.000182	864.616271	14.091482
17.704422	864.722786	14.096499
17.803553	861.438092	14.101517
17.884270	864.371493	14.106535
17.603078	865.681047	14.111552
17.835429	877.347178	14.116570
17.823634	883.355988	14.121587
18.012928	889.801165	14.126605
18.236958	886.975683	14.131623
18.066167	878.827257	14.136640
18.504829	864.526641	14.141658
17.990620	860.530951	14.146675
17.829972	861.882352	14.151693
17.810428	866.880285	14.156711
17.679264	854.805031	14.161728
17.850776	858.222190	14.166746
17.665601	867.723705	14.171763
18.148989	874.288673	14.176781
18.222904	882.745769	14.181799
18.402152	883.689331	14.186816
18.138246	865.500521	14.191834
17.990494	861.661068	14.196851
17.962789	860.531523	14.201869
18.137092	870.560493	14.206887
17.768239	889.273088	14.211904
18.055892	891.436043	14.216922
18.177467	892.403329	14.221939
18.345094	897.562789	14.226957
18.384490	893.918705	14.231975
18.291132	899.166655	14.236992
18.405935	894.135348	14.242010
18.155403	891.072713	14.247027
18.121287	896.467931	14.252045
18.026470	887.028635	14.257063
18.229931	897.196488	14.262080
18.447950	892.638223	14.267098
18.557050	892.421804	14.272115
18.372914	888.232481	14.277133
18.339213	896.507020	14.282151
18.347038	895.426311	14.287168
18.670387	883.039171	14.292186
18.224253	893.225220	14.297203
18.362302	880.072347	14.302221
18.624268	891.823738	14.307239
18.301134	898.971852	14.312256
18.603428	887.879078	14.317274
18.305192	892.054311	14.322291
18.624983	892.073858	14.327309
18.681374	893.287359	14.332327
18.324439	893.303221	14.337344
18.447916	890.113697	14.342362
18.368045	899.476934	14.347379
18.584494	897.297949	14.352397
18.617611	902.850139	14.357415
18.748027	921.349398	14.362432
18.925670	909.739873	14.367450
18.767539	906.321006	14.372467
18.458074	903.278363	14.377485
18.690888	909.782087	14.382503
18.739963	925.907137	14.387520
19.082785	916.537081	14.392538
19.085247	919.436208	14.397555
19.030154	909.748205	14.402573
19.143683	889.111547	14.407591
18.511082	895.516059	14.412608
18.742934	895.826139	14.417626
18.970569	905.075077	14.422643
19.000192	907.949626	14.427661
19.235729	902.039309	14.432679
18.877362	889.237908	14.437696
19.000215	888.588917	14.442714
19.102540	887.798451	14.447731
18.800334	892.249525	14.452749
19.364808	898.391648	14.457767
19.294041	891.408093	14.462784
18.928534	888.468822	14.467802
19.036690	884.581477	14.472819
19.082073	888.127790	14.477837
19.104202	878.446310	14.482855
19.072416	886.368576	14.487872
19.210570	901.432837	14.492890
19.202345	906.816292	14.497907
19.063368	913.271745	14.502925
19.462085	914.543518	14.507943
19.092289	909.174752	14.512960
19.259380	918.017600	14.517978
19.122390	912.535090	14.522995
19.091948	907.262880	14.528013
19.323453	911.925570	14.533031
19.331180	918.963397	14.538048
19.214641	915.972660	14.543066
19.403010	918.718568	14.548083
19.168023	914.737649	14.553101
19.421671	905.298905	14.558119
19.080937	919.025619	14.563136
19.123782	911.113047	14.568154
19.554054	919.093064	14.573171
19.262441	913.551122	14.578189
19.212433	910.823372	14.583207
19.325705	917.039428	14.588224
19.502955	910.170694	14.593242
19.289241	926.246350	14.598259
19.410637	939.282413	14.603277
19.523074	937.517873	14.608295
19.331328	945.494607	14.613312
19.592329	937.986824	14.618330
19.775569	937.666006	14.623347
19.555892	941.413695	14.628365
19.860144	936.604142	14.633383
19.488292	935.943764	14.638400
19.708479	930.973337	14.643418
19.653297	931.940367	14.648435
19.605472	939.295656	14.653453
19.898958	924.017102	14.658471
19.597646	940.181683	14.663488
19.448876	940.114652	14.668506
19.750466	938.062896	14.673523
19.529788	931.848207	14.678541
19.948251	939.231398	14.683559
20.150640	934.765863	14.688576
19.700502	930.289881	14.693594
19.906258	929.011835	14.698611
19.649617	938.709076	14.703629
20.099183	950.296777	14.708647
20.259552	957.847905	14.713664
20.664221	945.961794	14.718682
20.569821	937.162921	14.723699
20.326084	933.683423	14.728717
20.381249	925.916435	14.733735
20.453643	920.101232	14.738752
20.577532	918.522978	14.743770
20.466669	914.263250	14.748787
20.009864	904.263833	14.753805
20.214418	898.749968	14.758823
20.154777	903.284889	14.763840
20.096744	917.498230	14.768858
20.144720	922.537360	14.773875
19.820393	919.053100	14.778893
20.222146	923.698626	14.783911
20.029447	931.524731	14.788928
20.070171	924.594349	14.793946
20.671432	923.148062	14.798963
20.541291	922.909843	14.803981
20.478167	921.562547	14.808999
20.519754	930.542715	14.814016
20.353575	925.286283	14.819034
20.462530	914.451085	14.824051
20.248862	922.164520	14.829069
20.467594	920.676068	14.834087
20.571058	924.537561	14.839104
20.529718	914.733897	14.844122
20.674105	919.400385	14.849139
20.460687	927.371644	14.854157
20.286011	920.324970	14.859175
20.596773	920.318454	14.864192
20.538968	925.260146	14.869210
20.526742	923.313110	14.874227
20.328182	924.397578	14.879245
20.413039	919.785375	14.884263
20.335951	923.335048	14.889280
20.184224	928.384808	14.894298
21.051872	935.251512	14.899315
20.765627	940.063720	14.904333
20.624566	927.994772	14.909351
20.648657	934.787782	14.914368
20.966758	947.895214	14.919386
21.030239	947.295814	14.924403
20.518782	935.611014	14.929421
20.538153	941.585554	14.934439
20.583894	953.836162	14.939456
20.736969	954.265581	14.944474
21.136213	947.730134	14.949491
20.686972	953.688184	14.954509
20.800431	958.984582	14.959527
21.023188	950.760715	14.964544
21.073878	959.020133	14.969562
21.084925	953.375699	14.974579
20.661036	957.905206	14.979597
21.120823	950.503864	14.984615
21.057587	954.107941	14.989632
20.787769	956.667532	14.994650
21.015079	958.443656	14.999667
21.048702	959.084579	15.004685
21.027086	949.046929	15.009703
21.373033	947.383872	15.014720
21.231732	946.836885	15.019738
21.089991	951.102357	15.024755
21.005490	955.363076	15.029773
21.040741	976.173728	15.034791
21.495549	981.101419	15.039808
21.432512	987.911241	15.044826
21.720148	983.413467	15.049843
21.377578	966.756397	15.054861
21.505930	960.009906	15.059879
21.387087	952.854764	15.064896
21.666849	954.547402	15.069914
21.490813	936.487258	15.074931
21.488193	947.406166	15.079949
21.668209	945.595790	15.084967
21.334343	943.170144	15.089984
21.368507	956.063981	15.095002
21.489955	936.821950	15.100019
21.407953	943.671900	15.105037
21.510320	958.442550	15.110055
21.665507	958.224011	15.115072
21.523883	970.601322	15.120090
21.852660	970.722920	15.125107
21.777956	977.036660	15.130125
21.660791	954.266947	15.135143
21.748539	954.522546	15.140160
21.760355	958.233876	15.145178
21.730202	941.044808	15.150195
21.690987	952.252442	15.155213
21.763711	964.430483	15.160231
22.254268	955.688669	15.165248
21.947665	955.951302	15.170266
22.103114	946.090624	15.175283
21.902928	945.490398	15.180301
21.568316	939.093006	15.185319
21.386625	934.064720	15.190336
21.548405	957.971973	15.195354
21.996550	964.706195	15.200371
21.991730	973.219683	15.205389
22.105904	974.564955	15.210407
22.137840	972.022436	15.215424
22.240833	978.511861	15.220442
22.265856	967.314949	15.225459
22.210078	971.734689	15.230477
21.701883	964.347175	15.235495
22.065104	956.918515	15.240512
22.046847	972.399674	15.245530
22.296682	966.194458	15.250547
22.112500	968.126511	15.255565
21.982115	978.459536	15.260583
22.192490	979.432988	15.265600
22.205620	976.371164	15.270618
22.137525	967.251002	15.275635
22.010598	974.576494	15.280653
22.091836	980.549859	15.285671
22.161267	964.877675	15.290688
21.733395	980.858539	15.295706
22.152787	967.392482	15.300723
22.325881	976.709547	15.305741
22.347482	985.044658	15.310759
22.676745	987.940076	15.315776
22.888016	990.108606	15.320794
22.848340	971.725068	15.325811
22.683204	970.943848	15.330829
22.699095	968.163051	15.335847
22.800129	968.373933	15.340864
22.548645	965.469702	15.345882
22.540747	958.241070	15.350899
22.597140	964.235865	15.355917
22.957046	965.658552	15.360935
22.691339	958.159631	15.365952
22.475885	966.981210	15.370970
22.566980	956.744190	15.375987
22.471344	954.919225	15.381005
22.292648	965.755888	15.386023
22.430737	965.620098	15.391040
22.185525	991.472666	15.396058
22.583612	987.651061	15.401075
22.492852	998.205087	15.406093
22.777414	995.817182	15.411111
22.830166	980.546545	15.416128
22.990575	992.504586	15.421146
23.116439	988.574520	15.426163
22.898959	994.406024	15.431181
22.608766	990.211007	15.436199
23.105295	984.219255	15.441216
22.668489	987.906456	15.446234
22.820856	983.035822	15.451251
23.060302	1002.455274	15.456269
23.084244	1015.853195	15.461287
23.147768	1020.609085	15.466304
23.280235	1015.600797	15.471322
23.356903	1013.196527	15.476339
23.369791	1003.487367	15.481357
23.374267	992.495406	15.486375
23.270400	987.517599	15.491392
22.778429	983.918964	15.496410
23.201044	993.950596	15.501427
23.495931	1006.847758	15.506445
23.622615	1013.152573	15.511463
23.635871	992.044606	15.516480
23.014219	989.487480	15.521498
23.128370	983.216539	15.526515
23.390067	988.691148	15.531533
23.284523	1008.572047	15.536551
23.566929	1007.219494	15.541568
23.396947	1015.055658	15.546586
23.725332	1012.587661	15.551603
23.422594	1000.615898	15.556621
23.221666	1010.382302	15.561639
23.749084	1009.244680	15.566656
23.692411	1012.468958	15.571674
23.806173	1009.019613	15.576691
23.948448	995.846257	15.581709
23.383227	990.044487	15.586727
23.901437	976.714020	15.591744
23.457435	980.461858	15.596762
23.421253	993.130376	15.601779
23.935907	991.564571	15.606797
23.823431	1007.919205	15.611815
23.964566	1000.300537	15.616832
23.733271	996.774084	15.621850
23.998502	1001.358385	15.626867
23.891186	986.301248	15.631885
23.498298	987.530493	15.636903
23.528164	991.951804	15.641920
23.398377	1009.347846	15.646938
23.797623	1010.151055	15.651955
23.898469	992.156017	15.656973
23.691492	1007.900341	15.661991
23.675043	1005.974859	15.667008
23.757848	1003.837280	15.672026
23.869600	1011.085474	15.677043
24.262362	1019.164270	15.682061
24.137070	1038.358348	15.687079
24.324974	1027.788334	15.692096
24.113374	1018.333651	15.697114
24.258898	1014.585749	15.702131
24.228442	1005.188083	15.707149
24.063836	1006.470469	15.712167
24.240215	1014.639422	15.717184
24.209246	1031.844329	15.722202
24.542837	1034.565031	15.727219
24.583974	1026.373167	15.732237
23.900184	1015.293197	15.737255
24.789084	1014.539007	15.742272
24.227742	1018.159832	15.747290
24.561487	1025.428752	15.752307
24.895122	1016.286527	15.757325
24.351251	1012.565381	15.762343
24.459877	1000.318817	15.767360
24.193824	996.528839	15.772378
24.036091	1013.861406	15.777395
24.579021	1018.556416	15.782413
24.576479	1025.849919	15.787431
24.869325	1024.624371	15.792448
24.905609	1033.350763	15.797466
24.842008	1027.622603	15.802483
24.902353	1022.849474	15.807501
24.848814	1025.151226	15.812519
25.028473	1000.611496	15.817536
24.597340	1006.218550	15.822554
24.714947	999.495080	15.827571
24.815731	999.449715	15.832589
24.575966	1009.073736	15.837607
24.777274	1008.168059	15.842624
24.865497	1021.096304	15.847642
24.601486	1026.644985	15.852659
24.848987	1027.805987	15.857677
24.836719	1035.488491	15.862695
25.258461	1030.590166	15.867712
25.170878	1028.038296	15.872730
25.148838	1028.844732	15.877747
25.162995	1031.879340	15.882765
24.900421	1034.293656	15.887783
25.004784	1025.000814	15.892800
24.990610	1035.889809	15.897818
25.106121	1031.066599	15.902835
25.054187	1025.516029	15.907853
24.925813	1023.870879	15.912871
25.152469	1016.762036	15.917888
25.195802	1019.270965	15.922906
25.136650	1029.758758	15.927923
25.266739	1017.514925	15.932941
24.926020	1028.012727	15.937959
25.161783	1022.408221	15.942976
25.189128	1022.999007	15.947994
24.906509	1030.276687	15.953011
25.302253	1038.623887	15.958029
25.329905	1052.139725	15.963047
25.377494	1052.027974	15.968064
25.692107	1056.722615	15.973082
25.542243	1053.840908	15.978099
25.827415	1054.679937	15.983117
25.560729	1038.773188	15.988135
25.240975	1034.722024	15.993152
25.235713	1041.034920	15.998170
25.449684	1051.871582	16.003187
25.739711	1044.079030	16.008205
25.541815	1058.493999	16.013223
25.626208	1045.980162	16.018240
25.688726	1056.408457	16.023258
25.875225	1053.709627	16.028275
26.120450	1043.655288	16.033293
26.225802	1049.763265	16.038311
26.153809	1046.546236	16.043328
26.489259	1043.266466	16.048346
25.920671	1032.669750	16.053363
26.051896	1016.792013	16.058381
25.814076	1025.380330	16.063399
26.026467	1018.523052	16.068416
25.922441	1019.842256	16.073434
25.950879	1013.355190	16.078451
26.046914	1012.853543	16.083469
25.935128	1019.871838	16.088487
25.710237	1014.609350	16.093504
26.222768	1030.298727	16.098522
25.956544	1041.429847	16.103539
26.271295	1045.917382	16.108557
26.158130	1038.763622	16.113575
26.088326	1046.258422	16.118592
26.180028	1045.946068	16.123610
26.038860	1044.873090	16.128627
26.297981	1044.692850	16.133645
26.391184	1038.280873	16.138663
26.397882	1049.110911	16.143680
26.480871	1047.651617	16.148698
26.707742	1048.190863	16.153715
26.525500	1043.988191	16.158733
26.514301	1050.369788	16.163751
26.331331	1045.356638	16.168768
26.353385	1047.904527	16.173786
26.274480	1044.639826	16.178803
26.262496	1042.006146	16.183821
26.178674	1049.059979	16.188839
26.164122	1045.855092	16.193856
26.353632	1046.566660	16.198874
26.118862	1043.516738	16.203891
26.313584	1056.418717	16.208909
26.403482	1060.114386	16.213927
26.503759	1067.853465	16.218944
26.897546	1063.548713	16.223962
26.538036	1062.020569	16.228979
27.154604	1058.778101	16.233997
27.004832	1061.175317	16.239015
26.834370	1069.413541	16.244032
26.863753	1064.684108	16.249050
26.730376	1065.834561	16.254067
26.925678	1059.046627	16.259085
27.027588	1067.817681	16.264103
27.247753	1069.591458	16.269120
27.235099	1060.641187	16.274138
26.862797	1070.522224	16.279155
27.046309	1061.191452	16.284173
26.784846	1064.149662	16.289191
26.829029	1066.967109	16.294208
27.464882	1064.159226	16.299226
27.034546	1072.056245	16.304243
27.269052	1069.636855	16.309261
27.122458	1059.566679	16.314279
26.936474	1071.555368	16.319296
27.390438	1062.161309	16.324314
27.338348	1076.613567	16.329331
26.996781	1064.796603	16.334349
27.057702	1058.193907	16.339367
26.931977	1073.257939	16.344384
27.705581	1074.087349	16.349402
27.348206	1090.364910	16.354419
27.425181	1091.643126	16.359437
27.607106	1097.153030	16.364455
27.813187	1093.165168	16.369472
27.886988	1072.468311	16.374490
27.686720	1062.097977	16.379507
27.518076	1059.927621	16.384525
27.598404	1055.169676	16.389543
27.505486	1063.249393	16.394560
27.655861	1065.866585	16.399578
27.559091	1062.246978	16.404595
27.249710	1071.488485	16.409613
27.944966	1086.129983	16.414631
27.885078	1084.976617	16.419648
28.305756	1079.787912	16.424666
27.903098	1074.441851	16.429683
27.738204	1056.386808	16.434701
28.232480	1067.223521	16.439719
27.860427	1062.694807	16.444736
27.719856	1050.192627	16.449754
27.937575	1071.933789	16.454771
28.221491	1080.742033	16.459789
28.277257	1072.704409	16.464807
27.949260	1066.148787	16.469824
28.152999	1058.058717	16.474842
27.736571	1062.097272	16.479859
28.001632	1079.065820	16.484877
28.382760	1078.323664	16.489895
27.977030	1086.240237	16.494912
27.924826	1079.502726	16.499930
28.211301	1083.794569	16.504947
28.142551	1084.270959	16.509965
28.044823	1087.841409	16.514983
27.854092	1090.759174	16.520000
28.136698	1075.087404	16.525018
28.085141	1090.326566	16.530035
28.025399	1091.503016	16.535053
27.926474	1096.568890	16.540071
27.938530	1111.714864	16.545088
28.370982	1106.223424	16.550106
28.637414	1113.463769	16.555123
28.497752	1113.932218	16.560141
28.606570	1110.645868	16.565159
28.553135	1133.193406	16.570176
28.676368	1107.428638	16.575194
28.603538	1117.275470	16.580211
28.371095	1115.158975	16.585229
28.598465	1115.903252	16.590247
28.275505	1118.932677	16.595264
28.607879	1110.753959	16.600282
28.738945	1117.758856	16.605299
29.130962	1125.072109	16.610317
29.105104	1110.300173	16.615335
28.739805	1105.738833	16.620352
28.913671	1107.837592	16.625370
28.586483	1108.026473	16.630387
28.870513	1117.937832	16.635405
29.242557	1132.554550	16.640423
29.088446	1144.712027	16.645440
29.298390	1128.177855	16.650458
28.925232	1125.639398	16.655475
29.318012	1121.911944	16.660493
29.383883	1115.781616	16.665511
29.006051	1110.121993	16.670528
29.155248	1101.772043	16.675546
28.859117	1110.062987	16.680563
29.174334	1129.795633	16.685581
29.307062	1134.921583	16.690599
29.102548	1136.081852	16.695616
29.077878	1132.264469	16.700634
29.371712	1132.104856	16.705651
29.265580	1132.784282	16.710669
29.482340	1131.112679	16.715687
29.187781	1135.109027	16.720704
29.462816	1123.896193	16.725722
29.652924	1128.171329	16.730739
29.529226	1134.102313	16.735757
29.308670	1130.872466	16.740775
29.322992	1121.542903	16.745792
29.486694	1123.420127	16.750810
29.937245	1130.048122	16.755827
29.585521	1132.018174	16.760845
29.765542	1127.024809	16.765863
29.630732	1125.559448	16.770880
29.695243	1121.811156	16.775898
29.803117	1127.925832	16.780915
29.717178	1138.823239	16.785933
30.142972	1127.165375	16.790951
29.561600	1136.555891	16.795968
29.507985	1137.694717	16.800986
29.959498	1149.880653	16.806003
29.529762	1152.075823	16.811021
29.979009	1144.101350	16.816039
29.929494	1157.201724	16.821056
30.171869	1147.968237	16.826074
30.702084	1137.204070	16.831091
30.294087	1146.951699	16.836109
30.635795	1132.609414	16.841127
30.279181	1145.492134	16.846144
30.340214	1129.158202	16.851162
30.012975	1127.187713	16.856179
29.919058	1127.213563	16.861197
30.266532	1130.917384	16.866215
30.042075	1135.509978	16.871232
30.299766	1140.056201	16.876250
30.310481	1138.104158	16.881267
30.133531	1143.732555	16.886285
30.298352	1134.349718	16.891303
30.391181	1143.810880	16.896320
30.325323	1133.846181	16.901338
30.390489	1136.757800	16.906355
30.119936	1139.451790	16.911373
30.401986	1135.468661	16.916391
30.084422	1145.939875	16.921408
30.233113	1157.807861	16.926426
30.518043	1157.432407	16.931443
30.723676	1172.941258	16.936461
30.892531	1171.794496	16.941479
31.229032	1166.619308	16.946496
30.983256	1163.974321	16.951514
31.083426	1165.502239	16.956531
30.825780	1172.870729	16.961549
31.207848	1163.061756	16.966567
31.147108	1158.096043	16.971584
30.749506	1143.165558	16.976602
31.030087	1151.930696	16.981619
30.886331	1157.323294	16.986637
31.205709	1155.452025	16.991655
31.229228	1161.840124	16.996672
30.881741	1152.285027	17.001690
30.824725	1148.371818	17.006707
30.751261	1163.641844	17.011725
31.007083	1163.688520	17.016743
31.019158	1158.719805	17.021760
31.105037	1168.190006	17.026778
31.446383	1169.383509	17.031795
31.277973	1168.129213	17.036813
31.253719	1161.448454	17.041831
30.836027	1164.840414	17.046848
30.911786	1165.094066	17.051866
31.197127	1172.706493	17.056883
31.334888	1188.381319	17.061901
31.441421	1191.430189	17.066919
31.280206	1196.810732	17.071936
31.386733	1189.982718	17.076954
31.545393	1193.444205	17.081971
31.255606	1196.262646	17.086989
31.691985	1188.978451	17.092007
31.516013	1188.340348	17.097024
31.251955	1187.886904	17.102042
31.801429	1184.614972	17.107059
31.474704	1198.760860	17.112077
31.882005	1211.621470	17.117095
31.847526	1217.564090	17.122112
32.186173	1217.748622	17.127130
32.395098	1204.995144	17.132147
31.801006	1199.849630	17.137165
32.022264	1183.714301	17.142183
32.098812	1193.295508	17.147200
31.914827	1192.998879	17.152218
31.901508	1187.924914	17.157235
32.007250	1203.013341	17.162253
32.283053	1206.266856	17.167271
32.256973	1222.758982	17.172288
32.630716	1203.567754	17.177306
32.333375	1195.189335	17.182323
31.833468	1187.633415	17.187341
32.419364	1183.704289	17.192359
31.799557	1193.287419	17.197376
32.082679	1199.800259	17.202394
32.052178	1208.642530	17.207411
32.264042	1213.437301	17.212429
32.472305	1215.079605	17.217447
32.461724	1212.871636	17.222464
32.895214	1216.665957	17.227482
32.852732	1206.674900	17.232499
32.588073	1208.722668	17.237517
32.526450	1213.702878	17.242535
32.815403	1213.933434	17.247552
32.554505	1213.791269	17.252570
32.982606	1200.880246	17.257587
32.997693	1213.985718	17.262605
33.141768	1195.227008	17.267623
32.826378	1192.832513	17.272640
32.257653	1180.178295	17.277658
32.858829	1187.535290	17.282675
33.003123	1202.561822	17.287693
33.025677	1202.759719	17.292711
33.157798	1204.026452	17.297728
33.003415	1186.299035	17.302746
32.891443	1175.416775	17.307763
32.941818	1191.174969	17.312781
33.017519	1196.299752	17.317799
33.012073	1201.296640	17.322816
33.083212	1205.043087	17.327834
33.416599	1207.141823	17.332851
33.260454	1209.620823	17.337869
33.050847	1204.782105	17.342887
33.276312	1192.159754	17.347904
33.151079	1208.384432	17.352922
33.281229	1202.752074	17.357939
33.015426	1203.981944	17.362957
33.143093	1204.025432	17.367975
33.404375	1198.037514	17.372992
32.956082	1210.481150	17.378010
33.145443	1198.674985	17.383027
33.346095	1207.067968	17.388045
33.162920	1216.702431	17.393063
33.630664	1222.804799	17.398080
33.414439	1221.933603	17.403098
33.724481	1223.374020	17.408115
33.817885	1220.169724	17.413133
33.708108	1228.281846	17.418151
33.901664	1229.889580	17.423168
33.882041	1227.990185	17.428186
33.838351	1225.568018	17.433203
33.645962	1224.291310	17.438221
33.576776	1227.019686	17.443239
33.822715	1224.509405	17.448256
33.926715	1217.368027	17.453274
33.909911	1216.617348	17.458291
33.697313	1225.873235	17.463309
33.521910	1225.645262	17.468327
33.998958	1231.363426	17.473344
34.113631	1238.660061	17.478362
34.313316	1244.055662	17.483379
34.432500	1250.896843	17.488397
34.503985	1240.408559	17.493415
33.819321	1228.359311	17.498432
34.238344	1238.774366	17.503450
34.421587	1237.833873	17.508467
34.538644	1243.114419	17.513485
34.588945	1244.317146	17.518503
34.841188	1240.547975	17.523520
34.211444	1221.491392	17.528538
34.700772	1213.069314	17.533555
34.623584	1211.341260	17.538573
34.672159	1209.739229	17.543591
34.683416	1209.515780	17.548608
34.255935	1208.915385	17.553626
34.562599	1218.982899	17.558643
34.587343	1242.329047	17.563661
34.735814	1240.187650	17.568679
35.115320	1235.548217	17.573696
34.455047	1241.383055	17.578714
34.794271	1235.917242	17.583731
34.626215	1238.903718	17.588749
34.705167	1243.250047	17.593767
34.866257	1237.931443	17.598784
35.043907	1244.191695	17.603802
35.223307	1236.322880	17.608819
34.874014	1240.331073	17.613837
34.643408	1237.651279	17.618855
35.067613	1231.289135	17.623872
34.955509	1236.547783	17.628890
34.838008	1228.619475	17.633907
34.984432	1239.146596	17.638925
35.266832	1234.006327	17.643943
35.458004	1234.129061	17.648960
34.933257	1239.643434	17.653978
35.564287	1239.088232	17.658995
34.845138	1248.990200	17.664013
35.292438	1260.885984	17.669031
35.692331	1265.215789	17.674048
35.625891	1273.029426	17.679066
35.656477	1266.798192	17.684083
35.778008	1267.850547	17.689101
35.932893	1256.949632	17.694119
35.762458	1237.074473	17.699136
35.554352	1243.347419	17.704154
35.641686	1233.080132	17.709171
35.912007	1230.619748	17.714189
35.605145	1233.789439	17.719207
35.806906	1229.984537	17.724224
35.878021	1245.567703	17.729242
35.737323	1242.494684	17.734259
36.015778	1251.624395	17.739277
36.129342	1256.777574	17.744295
36.033590	1253.203422	17.749312
36.068618	1254.589776	17.754330
36.012972	1246.048082	17.759347
36.051253	1241.868288	17.764365
35.682926	1261.321777	17.769383
35.883190	1257.234052	17.774400
36.324687	1253.693378	17.779418
36.204609	1264.655580	17.784435
36.022945	1257.648490	17.789453
35.841691	1258.309652	17.794471
36.257383	1253.372104	17.799488
35.962583	1260.265696	17.804506
35.820322	1264.981329	17.809523
36.043191	1272.560058	17.814541
36.206640	1285.671339	17.819559
36.550683	1278.011850	17.824576
36.549109	1287.026930	17.829594
36.682088	1280.301975	17.834611
36.945718	1279.052900	17.839629
36.649316	1274.343096	17.844647
37.108420	1273.462433	17.849664
36.872011	1270.642258	17.854682
37.000159	1276.338686	17.859699
37.166045	1277.787624	17.864717
36.951430	1271.600926	17.869735
36.560705	1255.794016	17.874752
36.677758	1260.444663	17.879770
36.804703	1280.399223	17.884787
36.834098	1275.654370	17.889805
36.698016	1285.036595	17.894823
36.804676	1279.286842	17.899840
36.783312	1282.894692	17.904858
37.140105	1270.585169	17.909875
36.931450	1269.716652	17.914893
36.801082	1270.759538	17.919911
37.343651	1262.991201	17.924928
37.216475	1274.184500	17.929946
36.951929	1274.456315	17.934963
37.307393	1295.409646	17.939981
37.310868	1299.007087	17.944999
37.564134	1299.115210	17.950016
37.697670	1305.577275	17.955034
37.586284	1292.845268	17.960051
37.777734	1286.491328	17.965069
37.613449	1275.789309	17.970087
37.888692	1276.398111	17.975104
38.038476	1270.359338	17.980122
37.923817	1265.775738	17.985139
37.924981	1268.410586	17.990157
37.776991	1267.773751	17.995175
37.660378	1256.266626	18.000192
37.795251	1269.948754	18.005210
37.871518	1273.581773	18.010227
38.020864	1276.497590	18.015245
37.420153	1274.016077	18.020263
37.767199	1267.868659	18.025280
37.795996	1265.941163	18.030298
37.809083	1269.962587	18.035315
38.020002	1284.809274	18.040333
37.964629	1297.535155	18.045351
38.253961	1290.509508	18.050368
37.685445	1303.976253	18.055386
37.918703	1297.093350	18.060403
38.323320	1291.723775	18.065421
37.971529	1306.203825	18.070439
38.288472	1302.303457	18.075456
38.154479	1298.952944	18.080474
38.361401	1294.028299	18.085491
38.299413	1298.283415	18.090509
38.388641	1298.222248	18.095527
38.614831	1305.557928	18.100544
38.638860	1328.712203	18.105562
38.463950	1329.641997	18.110579
38.624249	1318.194878	18.115597
38.793074	1323.483809	18.120615
38.628735	1321.469391	18.125632
38.901110	1323.558169	18.130650
38.771532	1315.749136	18.135667
38.941056	1326.994131	18.140685
38.862475	1320.357337	18.145703
38.999392	1317.234792	18.150720
38.685109	1322.073412	18.155738
38.719130	1315.740016	18.160755
38.774589	1314.868708	18.165773
38.759835	1320.258506	18.170791
39.056431	1316.896532	18.175808
39.007870	1314.199573	18.180826
38.529541	1319.199211	18.185843
38.918353	1332.039756	18.190861
38.980837	1348.265387	18.195879
39.143265	1348.260994	18.200896
39.236491	1352.347121	18.205914
39.142128	1351.766362	18.210931
39.515501	1343.041768	18.215949
39.214342	1341.387004	18.220967
39.421721	1338.003973	18.225984
39.688947	1341.836880	18.231002
39.856048	1349.101658	18.236019
39.756364	1333.624029	18.241037
39.456628	1338.740948	18.246055
39.737854	1344.638034	18.251072
39.885262	1336.143769	18.256090
39.436640	1338.856255	18.261107
39.761379	1337.177380	18.266125
39.627944	1340.950647	18.271143
39.999587	1336.762085	18.276160
40.053608	1335.201657	18.281178
40.059272	1333.250032	18.286195
40.082116	1329.501896	18.291213
39.844822	1348.105860	18.296231
39.755412	1331.410019	18.301248
39.925220	1339.357009	18.306266
39.723512	1346.449787	18.311283
40.246331	1360.009885	18.316301
40.398582	1366.179118	18.321319
40.642850	1364.303333	18.326336
40.625748	1347.421095	18.331354
40.313136	1345.579648	18.336371
40.307554	1338.665410	18.341389
39.996485	1348.198300	18.346407
40.381882	1350.912449	18.351424
40.775504	1366.037225	18.356442
40.318071	1371.255856	18.361459
40.769013	1365.538039	18.366477
40.885060	1371.717600	18.371495
40.782480	1360.308073	18.376512
40.553019	1362.896085	18.381530
40.169729	1360.365171	18.386547
40.769206	1356.945950	18.391565
40.603985	1362.006747	18.396583
40.652644	1359.322815	18.401600
40.590400	1360.774891	18.406618
40.316478	1365.680462	18.411635
40.892185	1361.607314	18.416653
41.037754	1374.075973	18.421671
40.933728	1383.989556	18.426688
40.991223	1384.499381	18.431706
41.104462	1392.381356	18.436723
41.295475	1387.015228	18.441741
40.963496	1389.005270	18.446759
41.396570	1388.042298	18.451776
41.309251	1383.801769	18.456794
41.249636	1378.082268	18.461811
41.297772	1370.452045	18.466829
41.133852	1377.366537	18.471847
41.540947	1381.328260	18.476864
41.916481	1382.411004	18.481882
41.494986	1381.640321	18.486899
41.335250	1374.881905	18.491917
41.470772	1383.440490	18.496935
41.539075	1373.632946	18.501952
41.998572	1379.510763	18.506970
41.522878	1376.678616	18.511987
41.494969	1376.171104	18.517005
41.672569	1379.329502	18.522023
41.844414	1396.947683	18.527040
42.239601	1400.140528	18.532058
41.911006	1412.624740	18.537075
42.209637	1409.057689	18.542093
42.190771	1406.327450	18.547111
42.098341	1405.047954	18.552128
42.442915	1401.704396	18.557146
41.929550	1383.563366	18.562163
42.242900	1394.044842	18.567181
42.075731	1399.184319	18.572199
42.237673	1405.979513	18.577216
42.239679	1401.280494	18.582234
41.916456	1418.062183	18.587251
42.100904	1411.482189	18.592269
42.048009	1411.524474	18.597287
41.780821	1411.643581	18.602304
42.104521	1412.820735	18.607322
42.107129	1433.993703	18.612339
42.622700	1438.458339	18.617357
42.632861	1431.925699	18.622375
42.512807	1438.381386	18.627392
42.855873	1427.118488	18.632410
42.920615	1433.549478	18.637427
42.959725	1431.942692	18.642445
43.049407	1422.587477	18.647463
42.861593	1437.960171	18.652480
42.917978	1430.587211	18.657498
42.971320	1428.460753	18.662515
43.248330	1433.740075	18.667533
42.998158	1429.438311	18.672551
43.101977	1420.985075	18.677568
43.283753	1420.688113	18.682586
43.435768	1419.247670	18.687603
43.538543	1418.116163	18.692621
43.297759	1424.461127	18.697639
43.046409	1413.972245	18.702656
43.397209	1410.444585	18.707674
42.996947	1413.529779	18.712691
43.143835	1417.306253	18.717709
43.707735	1406.584749	18.722727
43.264485	1414.853758	18.727744
43.371071	1413.687369	18.732762
43.314061	1438.139066	18.737779
43.656318	1443.411919	18.742797
43.819030	1449.360165	18.747815
43.646399	1449.379757	18.752832
44.059362	1443.822529	18.757850
43.808406	1447.722367	18.762867
43.956994	1447.967508	18.767885
43.983491	1447.933262	18.772903
43.692389	1447.928377	18.777920
44.233461	1452.984457	18.782938
44.314680	1436.045291	18.787955
44.013501	1439.828248	18.792973
43.980543	1445.056932	18.797991
43.958530	1446.138186	18.803008
44.563380	1434.917367	18.808026
44.065882	1447.572093	18.813043
43.994152	1442.031343	18.818061
44.400373	1445.734570	18.823079
44.176299	1447.167781	18.828096
44.410316	1440.103590	18.833114
44.146090	1455.818477	18.838131
44.567130	1459.388940	18.843149
44.515445	1458.872369	18.848167
44.406855	1462.943517	18.853184
44.779174	1454.876115	18.858202
44.535043	1465.013733	18.863219
44.357991	1463.122266	18.868237
44.879916	1461.796945	18.873255
44.835516	1465.547626	18.878272
45.086676	1453.875521	18.883290
44.901953	1464.880458	18.888307
44.779781	1460.513003	18.893325
44.866458	1457.944411	18.898343
44.766584	1464.433380	18.903360
45.235093	1473.889625	18.908378
45.298366	1482.229127	18.913395
45.095446	1476.799851	18.918413
45.374778	1479.522138	18.923431
45.211949	1487.648297	18.928448
45.646989	1478.301611	18.933466
45.343609	1476.807435	18.938483
45.644168	1477.024263	18.943501
45.676760	1456.275449	18.948519
45.453908	1455.854543	18.953536
45.316578	1449.899855	18.958554
45.421508	1458.896613	18.963571
45.856478	1475.166999	18.968589
45.496776	1478.013207	18.973607
45.549643	1484.262329	18.978624
45.586876	1487.094389	18.983642
45.879285	1487.862168	18.988659
45.864075	1489.795440	18.993677
45.521199	1479.903552	18.998695
45.874993	1488.747310	19.003712
45.957860	1476.327472	19.008730
46.010570	1484.089991	19.013747
45.645323	1487.683962	19.018765
46.022879	1477.425544	19.023783
45.856863	1489.741561	19.028800
45.920321	1506.728213	19.033818
46.340937	1508.717275	19.038835
46.073174	1503.000697	19.043853
46.365292	1511.225552	19.048871
46.419687	1512.289040	19.053888
46.448396	1505.397002	19.058906
46.382234	1503.216700	19.063923
46.416381	1514.870071	19.068941
46.471044	1503.728887	19.073959
46.421852	1501.028062	19.078976
46.328173	1504.507387	19.083994
46.794394	1514.248284	19.089011
46.583436	1525.460362	19.094029
46.519666	1524.119418	19.099047
46.930341	1526.823115	19.104064
47.224929	1517.277223	19.109082
47.115728	1518.124889	19.114099
47.163736	1518.662667	19.119117
47.498598	1524.308817	19.124135
47.206744	1525.434363	19.129152
47.385128	1516.571881	19.134170
47.582135	1524.136512	19.139187
47.611233	1516.017248	19.144205
47.396163	1496.148359	19.149223
47.014826	1495.098975	19.154240
47.339634	1506.411302	19.159258
47.405943	1517.166443	19.164275
47.483394	1514.867871	19.169293
47.750330	1515.969789	19.174311
47.522563	1519.483524	19.179328
47.575361	1513.401661	19.184346
47.773389	1521.013759	19.189363
47.283006	1522.873747	19.194381
47.695512	1518.022077	19.199399
47.563981	1525.598589	19.204416
47.532630	1515.636591	19.209434
47.674665	1507.320287	19.214451
47.795141	1524.016023	19.219469
48.156524	1528.384564	19.224487
48.055244	1539.870616	19.229504
48.349376	1540.903859	19.234522
48.704582	1526.252285	19.239539
48.389963	1520.732828	19.244557
48.401675	1514.082575	19.249575
48.232283	1513.333133	19.254592
48.269097	1510.742080	19.259610
48.555633	1503.195939	19.264627
48.351356	1508.427028	19.269645
48.179226	1500.665892	19.274663
48.241181	1524.077563	19.279680
48.490424	1527.434757	19.284698
48.687323	1528.788429	19.289715
48.376411	1537.740309	19.294733
48.825732	1531.641601	19.299751
48.313167	1536.493040	19.304768
48.127426	1538.512428	19.309786
48.407671	1539.860568	19.314803
48.437419	1536.176199	19.319821
48.574055	1552.622836	19.324839
48.612701	1568.940046	19.329856
48.741785	1565.898275	19.334874
48.794797	1571.291506	19.339891
49.200495	1570.700773	19.344909
49.545537	1559.335879	19.349927
49.334101	1568.395714	19.354944
49.154793	1565.130599	19.359962
49.398075	1561.260474	19.364979
49.269561	1557.566479	19.369997
49.100828	1561.875957	19.375015
49.075330	1565.686130	19.380032
49.267098	1581.829182	19.385050
49.706476	1589.841507	19.390067
49.732342	1585.981392	19.395085
50.028334	1583.245051	19.400103
49.979963	1587.908227	19.405120
49.928272	1588.674327	19.410138
50.065423	1581.382804	19.415155
49.721575	1586.979942	19.420173
49.777491	1577.768806	19.425191
49.978482	1585.679658	19.430208
49.645187	1589.000252	19.435226
50.056846	1580.975483	19.440243
49.471635	1589.385019	19.445261
50.029229	1575.175083	19.450279
49.726670	1589.642914	19.455296
50.127586	1609.696236	19.460314
50.765109	1607.041135	19.465331
50.499955	1623.828785	19.470349
50.694069	1609.314437	19.475367
50.942746	1603.649711	19.480384
50.873986	1596.793850	19.485402
51.175690	1574.881422	19.490419
50.568681	1578.363871	19.495437
50.791257	1572.066472	19.500455
50.780824	1572.502513	19.505472
50.800825	1580.079945	19.510490
51.124046	1567.978502	19.515507
50.860093	1568.594315	19.520525
50.940183	1562.935864	19.525543
50.683828	1566.709854	19.530560
50.683254	1571.660385	19.535578
51.270366	1569.493951	19.540595
50.895390	1598.016644	19.545613
51.629251	1590.029858	19.550631
51.162500	1594.970973	19.555648
51.049674	1604.177493	19.560666
51.485423	1599.838090	19.565683
51.554998	1598.314431	19.570701
51.357607	1602.672759	19.575719
51.374729	1602.176680	19.580736
51.530342	1599.440352	19.585754
51.287339	1597.012546	19.590771
51.313510	1604.171646	19.595789
51.546978	1598.592117	19.600807
51.444895	1596.623654	19.605824
51.165651	1605.100646	19.610842
51.618764	1611.763467	19.615859
51.505043	1611.802438	19.620877
51.597944	1616.390656	19.625895
52.003210	1619.654321	19.630912
51.902319	1620.025419	19.635930
51.902540	1615.478599	19.640947
51.933524	1626.823917	19.645965
51.939136	1618.893921	19.650983
52.080931	1625.614989	19.656000
51.877725	1645.799491	19.661018
52.289633	1646.654579	19.666035
52.298635	1655.589776	19.671053
52.516004	1647.936908	19.676071
52.471265	1643.908154	19.681088
52.602077	1651.327116	19.686106
52.992418	1642.130253	19.691123
52.788598	1647.616825	19.696141
52.886879	1656.173066	19.701159
52.912278	1641.540954	19.706176
52.715172	1648.972872	19.711194
52.860340	1642.931963	19.716211
53.090617	1653.033278	19.721229
53.021828	1650.365199	19.726247
52.900786	1645.232149	19.731264
52.973179	1652.194248	19.736282
53.348549	1644.954196	19.741299
53.104435	1649.307282	19.746317
53.249282	1648.856195	19.751335
53.273745	1641.063618	19.756352
53.064834	1642.464020	19.761370
53.363532	1636.273677	19.766387
53.556497	1644.552817	19.771405
53.362369	1631.527931	19.776423
53.534836	1640.888022	19.781440
53.066253	1647.640480	19.786458
53.376363	1643.292735	19.791475
53.305531	1661.896676	19.796493
53.409763	1666.218466	19.801511
53.788857	1666.411664	19.806528
53.695675	1674.872846	19.811546
53.857942	1669.393271	19.816563
53.825261	1665.908185	19.821581
53.903020	1684.193061	19.826599
54.273435	1688.289285	19.831616
54.284067	1700.496692	19.836634
54.695329	1685.437654	19.841651
54.454007	1676.948514	19.846669
54.288427	1665.312183	19.851687
54.531716	1654.106982	19.856704
54.328537	1663.722987	19.861722
54.447769	1647.870999	19.866739
54.082790	1660.916553	19.871757
54.577757	1680.390613	19.876775
54.688906	1682.207317	19.881792
54.991918	1687.343052	19.886810
54.819399	1683.987022	19.891827
54.703212	1687.760273	19.896845
54.879274	1685.297711	19.901863
55.383768	1682.687459	19.906880
55.361246	1684.218815	19.911898
55.263027	1679.899693	19.916915
55.022718	1674.338742	19.921933
55.080217	1674.212748	19.926951
55.139882	1677.182074	19.931968
55.166933	1686.515089	19.936986
54.909875	1683.691170	19.942003
54.964555	1683.369973	19.947021
54.743376	1683.903510	19.952039
55.256709	1689.905211	19.957056
55.171764	1685.244519	19.962074
55.100797	1694.166602	19.967091
55.146347	1700.345369	19.972109
55.151981	1711.195731	19.977127
55.485696	1705.529092	19.982144
55.134386	1709.342067	19.987162
55.376291	1713.628475	19.992179
55.411869	1730.451879	19.997197
55.418969	1740.676818	20.002215
55.748101	1739.084577	20.007232
55.429723	1739.239326	20.012250
55.731554	1755.415123	20.017267
55.928944	1763.370362	20.022285
56.046226	1762.911238	20.027303
56.501421	1759.742991	20.032320
56.206206	1768.488859	20.037338
55.995996	1760.690590	20.042355
56.706651	1763.661592	20.047373
56.773985	1758.201248	20.052391
56.761029	1755.125084	20.057408
56.391533	1762.888753	20.062426
56.723902	1753.845126	20.067443
56.888921	1746.750882	20.072461
56.576422	1753.939750	20.077479
57.076822	1742.870260	20.082496
56.705649	1753.494852	20.087514
56.916465	1749.081234	20.092531
56.744166	1751.768114	20.097549
57.426482	1745.063024	20.102567
57.220855	1736.697469	20.107584
57.123710	1740.316397	20.112602
57.331454	1745.025009	20.117619
57.191244	1748.519573	20.122637
56.990629	1752.970210	20.127655
57.572157	1760.255145	20.132672
57.380416	1764.971247	20.137690
57.633105	1773.972070	20.142707
57.540819	1779.156753	20.147725
57.062256	1782.199863	20.152743
57.613376	1774.008989	20.157760
57.670862	1773.903469	20.162778
58.106151	1775.390133	20.167795
57.875361	1772.302003	20.172813
57.885970	1781.355512	20.177831
58.015024	1773.266807	20.182848
57.494480	1786.338617	20.187866
57.648310	1778.341478	20.192883
57.612827	1785.478587	20.197901
57.555339	1808.736054	20.202919
57.964828	1796.692985	20.207936
58.086728	1798.806351	20.212954
58.250452	1796.546603	20.217971
58.094325	1789.078739	20.222989
58.108614	1812.008181	20.228007
58.337622	1823.406682	20.233024
58.374761	1824.471474	20.238042
58.618343	1830.689552	20.243059
58.906065	1816.907946	20.248077
58.688090	1818.956329	20.253095
59.157388	1815.158563	20.258112
58.926668	1824.719384	20.263130
59.133978	1826.579632	20.268147
59.022889	1815.925911	20.273165
59.122715	1820.552808	20.278183
59.325211	1814.080681	20.283200
59.043065	1820.238558	20.288218
59.389134	1819.145873	20.293235
59.451860	1823.539147	20.298253
59.277816	1828.545255	20.303271
59.747665	1826.466314	20.308288
59.348664	1829.815161	20.313306
59.449581	1815.248729	20.318323
59.642769	1821.924759	20.323341
59.610886	1817.229256	20.328359
59.760621	1816.394280	20.333376
59.793723	1815.604207	20.338394
59.487884	1819.390781	20.343411
59.832236	1816.755055	20.348429
59.267037	1818.390453	20.353447
59.888906	1831.853859	20.358464
59.944522	1842.554303	20.363482
59.786801	1848.660092	20.368499
60.143779	1854.320025	20.373517
60.073251	1847.266705	20.378535
60.460570	1846.501446	20.383552
59.856052	1842.651549	20.388570
59.783631	1848.350689	20.393587
60.329752	1856.996670	20.398605
60.065027	1870.241944	20.403623
60.344539	1875.599746	20.408640
60.604757	1870.966493	20.413658
60.542524	1875.581263	20.418675
60.804545	1866.941745	20.423693
60.267552	1878.773423	20.428711
61.005699	1878.705597	20.433728
60.695180	1880.011819	20.438746
61.051697	1883.822597	20.443763
61.220348	1893.874823	20.448781
60.871732	1902.198499	20.453799
61.138034	1899.828837	20.458816
61.583691	1904.116208	20.463834
61.287064	1894.577818	20.468851
61.497709	1885.968844	20.473869
61.459615	1894.827724	20.478887
61.347572	1892.633309	20.483904
61.391848	1896.598942	20.488922
61.090036	1896.512755	20.493939
61.564171	1888.903476	20.498957
61.288041	1903.161706	20.503975
61.778350	1906.446392	20.508992
61.661050	1919.871631	20.514010
61.662671	1921.175780	20.519027
62.053215	1913.935455	20.524045
61.829805	1917.835966	20.529063
62.212163	1913.749417	20.534080
62.117144	1914.463256	20.539098
62.077907	1918.037597	20.544115
62.387874	1905.002244	20.549133
62.245080	1906.985040	20.554151
62.363477	1907.712756	20.559168
62.528811	1917.689561	20.564186
62.448219	1925.883829	20.569203
63.061987	1931.546943	20.574221
62.448307	1931.996655	20.579239
62.613097	1922.387360	20.584256
62.698145	1936.014547	20.589274
62.540647	1939.864779	20.594291
63.377185	1924.039018	20.599309
63.433408	1932.227172	20.604327
63.233548	1919.258900	20.609344
63.137349	1924.947438	20.614362
62.701992	1939.996647	20.619379
62.757643	1932.787748	20.624397
63.027427	1935.990447	20.629415
63.383757	1937.859894	20.634432
63.438345	1933.536267	20.639450
63.177315	1929.375532	20.644467
63.113431	1932.663401	20.649485
63.250646	1950.165896	20.654503
63.500929	1950.068611	20.659520
63.554813	1955.422854	20.664538
63.559332	1968.920881	20.669555
63.809547	1966.057405	20.674573
63.639852	1961.598462	20.679591
63.713911	1962.854399	20.684608
63.779921	1966.738497	20.689626
63.494760	1986.701178	20.694643
64.014200	1988.592838	20.699661
63.961402	1991.028076	20.704679
63.683728	1989.761093	20.709696
64.255385	1993.859119	20.714714
63.957809	2000.740504	20.719731
64.497697	2012.154207	20.724749
64.394269	2029.750575	20.729767
64.762135	2024.352190	20.734784
64.735110	2013.249364	20.739802
64.644594	2024.677690	20.744819
65.119430	2010.920445	20.749837
64.708706	2011.920033	20.754855
65.137191	2019.915489	20.759872
65.010051	2017.310553	20.764890
65.323274	2007.641589	20.769907
65.482867	2014.840994	20.774925
65.464288	2021.557685	20.779943
65.317362	2007.472279	20.784960
65.471873	2007.382583	20.789978
65.575226	2014.644057	20.794995
65.755576	2006.657764	20.800013
65.435196	2015.557547	20.805031
65.674091	2011.352991	20.810048
65.793384	2004.986297	20.815066
65.523191	2011.832837	20.820083
65.550319	1999.367085	20.825101
65.738686	1999.325328	20.830119
65.733612	2001.526676	20.835136
65.678616	2001.551593	20.840154
65.912629	2006.018922	20.845171
65.950042	2015.602394	20.850189
66.149531	2033.152154	20.855207
66.177236	2028.103799	20.860224
66.330900	2027.385094	20.865242
65.893303	2034.972372	20.870259
66.131794	2027.234323	20.875277
66.146343	2024.579547	20.880295
66.412654	2035.603515	20.885312
66.855482	2032.397497	20.890330
66.771035	2035.266734	20.895347
67.026398	2028.118820	20.900365
66.731244	2032.278882	20.905383
66.806310	2037.433579	20.910400
67.024978	2049.526890	20.915418
66.778897	2064.486217	20.920435
67.015846	2059.085874	20.925453
66.800429	2053.735237	20.930471
66.794746	2061.004943	20.935488
67.287974	2050.323837	20.940506
67.090548	2061.086409	20.945523
67.034013	2050.047893	20.950541
67.059510	2066.204808	20.955559
67.406487	2077.155211	20.960576
67.841404	2074.778078	20.965594
67.556331	2090.133660	20.970611
67.488527	2083.731769	20.975629
67.557960	2081.155694	20.980647
67.381271	2080.590900	20.985664
67.820365	2088.467703	20.990682
67.852899	2099.385145	20.995699
67.929239	2111.857594	21.000717
68.087230	2105.860447	21.005735
68.101831	2102.807212	21.010752
68.523184	2096.747565	21.015770
68.493344	2104.261456	21.020787
68.705072	2097.532558	21.025805
68.634144	2098.094381	21.030823
68.525186	2103.018538	21.035840
69.028232	2093.735426	21.040858
68.818576	2095.278909	21.045875
68.610677	2095.436626	21.050893
68.680814	2092.751768	21.055911
68.637418	2094.973255	21.060928
69.042125	2095.637826	21.065946
68.662956	2101.433912	21.070963
68.946333	2090.115458	21.075981
69.017272	2100.886380	21.080999
68.681340	2126.005047	21.086016
69.220285	2120.692086	21.091034
69.018610	2120.986966	21.096051
69.006991	2124.174093	21.101069
69.134681	2120.077293	21.106087
69.278128	2126.232934	21.111104
69.567598	2135.981051	21.116122
69.760264	2146.016866	21.121139
70.068217	2135.416381	21.126157
70.201993	2139.321587	21.131175
70.165174	2142.101065	21.136192
70.480087	2135.945637	21.141210
70.659145	2137.578310	21.146227
70.180468	2122.878022	21.151245
70.299231	2111.259632	21.156263
70.271484	2107.628351	21.161280
70.626524	2118.173499	21.166298
70.338083	2134.796651	21.171315
70.508489	2132.317632	21.176333
70.651510	2130.828219	21.181351
70.478070	2132.988957	21.186368
70.792041	2129.855439	21.191386
70.485575	2139.027012	21.196403
70.749839	2140.087292	21.201421
70.802537	2137.037585	21.206439
70.388239	2139.603177	21.211456
70.773453	2141.426133	21.216474
71.007940	2151.564479	21.221491
71.205664	2151.069584	21.226509
71.049688	2148.456801	21.231527
71.109175	2159.995828	21.236544
71.039261	2155.511645	21.241562
71.034239	2157.315356	21.246579
71.149486	2166.334046	21.251597
71.560480	2185.229714	21.256615
71.410506	2194.251388	21.261632
71.584852	2181.339446	21.266650
71.820635	2192.386297	21.271667
71.622936	2190.478473	21.276685
71.999361	2189.356722	21.281703
71.702226	2187.894511	21.286720
72.342041	2204.854611	21.291738
72.018851	2216.718074	21.296755
72.520243	2211.868798	21.301773
72.633141	2214.879809	21.306791
72.413005	2210.927982	21.311808
72.845542	2203.884516	21.316826
72.575795	2202.385090	21.321843
72.682778	2204.152150	21.326861
73.138820	2208.378831	21.331879
72.692298	2193.104627	21.336896
72.677314	2186.082509	21.341914
72.555487	2185.943288	21.346931
72.535321	2200.804313	21.351949
73.129314	2204.275448	21.356967
72.761445	2207.926317	21.361984
72.901123	2198.428101	21.367002
73.136032	2202.829588	21.372019
72.744213	2204.496554	21.377037
73.055688	2221.097635	21.382055
72.969599	2236.974372	21.387072
73.474941	2229.653475	21.392090
73.471617	2229.839922	21.397107
73.398256	2226.750831	21.402125
73.822501	2222.069056	21.407143
73.814251	2236.417099	21.412160
74.139116	2236.880322	21.417178
74.029304	2254.893372	21.422195
73.799080	2251.233374	21.427213
74.173801	2244.088828	21.432231
74.181489	2257.571226	21.437248
74.519551	2238.358255	21.442266
74.403686	2246.406952	21.447283
74.333174	2244.739882	21.452301
74.839742	2246.091954	21.457319
74.722406	2244.568864	21.462336
74.640492	2239.607490	21.467354
74.711889	2250.485531	21.472371
74.824073	2248.201968	21.477389
75.157830	2241.892979	21.482407
74.818116	2242.584748	21.487424
74.988964	2238.486678	21.492442
75.030156	2237.243257	21.497459
74.859015	2236.073972	21.502477
75.240570	2249.674782	21.507495
75.152937	2266.612871	21.512512
75.426815	2270.022059	21.517530
75.278510	2266.145336	21.522547
75.162562	2274.636598	21.527565
75.436936	2272.828167	21.532583
75.443362	2270.362497	21.537600
75.467248	2280.031446	21.542618
75.888842	2286.709230	21.547635
75.696076	2303.473814	21.552653
75.850999	2299.743735	21.557671
75.950244	2298.408804	21.562688
76.009228	2300.986220	21.567706
76.160512	2294.797584	21.572723
76.065727	2292.592379	21.577741
76.222562	2282.616842	21.582759
76.251660	2312.138548	21.587776
76.556596	2322.711030	21.592794
76.729725	2314.678924	21.597811
76.768253	2314.922618	21.602829
76.925675	2315.061977	21.607847
76.973159	2320.553240	21.612864
76.867537	2321.371613	21.617882
76.584849	2314.113828	21.622899
76.645579	2321.380928	21.627917
76.709413	2312.304274	21.632935
76.764240	2333.140280	21.637952
76.945958	2347.020337	21.642970
77.436436	2341.825963	21.647987
77.222613	2346.000201	21.653005
77.423366	2338.694645	21.658023
77.365978	2337.872675	21.663040
77.436142	2337.704027	21.668058
77.832495	2354.566013	21.673075
78.050894	2366.611190	21.678093
78.353676	2351.589159	21.683111
77.946353	2349.618380	21.688128
77.801496	2336.527654	21.693146
77.781992	2347.037331	21.698163
77.787257	2361.798232	21.703181
78.338774	2362.675921	21.708199
78.381876	2369.864069	21.713216
78.340057	2356.933045	21.718234
78.550628	2354.526872	21.723251
78.351680	2363.112638	21.728269
78.679539	2355.383253	21.733287
78.530859	2357.971438	21.738304
78.672558	2378.587206	21.743322
78.910913	2378.258813	21.748339
78.900606	2389.982803	21.753357
78.888221	2381.572304	21.758375
79.018941	2384.378418	21.763392
78.877237	2382.933368	21.768410
79.226220	2374.138221	21.773427
79.034045	2389.362174	21.778445
79.613262	2393.887032	21.783463
79.649333	2412.523779	21.788480
79.728637	2411.266555	21.793498
79.900589	2408.531318	21.798515
79.978283	2411.627334	21.803533
80.288707	2406.081629	21.808551
80.112393	2405.405338	21.813568
79.910413	2408.853186	21.818586
80.065236	2394.915114	21.823603
80.174575	2401.732449	21.828621
80.644073	2392.618110	21.833639
80.499079	2403.652565	21.838656
80.242761	2401.720560	21.843674
80.399027	2394.048309	21.848691
80.309347	2394.469539	21.853709
80.485998	2393.546608	21.858727
80.490481	2399.446613	21.863744
80.714821	2409.831702	21.868762
81.174117	2411.234532	21.873779
80.844011	2425.416738	21.878797
81.440427	2411.386636	21.883815
81.281656	2417.937725	21.888832
81.204703	2414.862578	21.893850
81.338434	2423.315337	21.898867
81.183637	2424.801340	21.903885
81.400490	2405.707057	21.908903
81.598885	2422.870806	21.913920
81.436890	2413.575171	21.918938
81.620539	2415.446497	21.923955
81.181863	2427.639493	21.928973
81.704646	2439.539049	21.933991
81.643083	2448.070222	21.939008
81.585470	2445.514729	21.944026
82.045614	2443.881042	21.949043
81.831332	2445.393039	21.954061
81.933426	2460.477783	21.959079
82.342686	2473.110765	21.964096
82.227551	2476.218247	21.969114
82.408883	2473.149932	21.974131
82.275796	2476.665527	21.979149
82.520943	2477.853413	21.984167
82.642322	2477.593996	21.989184
82.740372	2498.010445	21.994202
83.365058	2491.709882	21.999219
82.822615	2499.252928	22.004237
83.211092	2492.506409	22.009255
83.155021	2496.861272	22.014272
83.225238	2499.008096	22.019290
83.437289	2488.947690	22.024307
83.324352	2501.321468	22.029325
83.028336	2499.409804	22.034343
83.526882	2499.720650	22.039360
83.042409	2502.992838	22.044378
83.805268	2503.588680	22.049395
83.742975	2515.139078	22.054413
83.715019	2520.273196	22.059431
83.790701	2510.792079	22.064448
83.919530	2513.916265	22.069466
84.156809	2508.053483	22.074483
83.919686	2506.213173	22.079501
84.151578	2507.714691	22.084519
84.484338	2508.364816	22.089536
84.378899	2530.907638	22.094554
84.656637	2527.851305	22.099571
84.565269	2532.900645	22.104589
84.986557	2537.367044	22.109607
84.804422	2537.051180	22.114624
84.425075	2538.598784	22.119642
85.305698	2535.878481	22.124659
85.131881	2541.458434	22.129677
85.076420	2537.872587	22.134695
85.298654	2537.741360	22.139712
85.294457	2539.889093	22.144730
85.397143	2540.844258	22.149747
85.073132	2540.199108	22.154765
85.580558	2554.014792	22.159783
85.472741	2556.397020	22.164800
85.480794	2566.137276	22.169818
85.730243	2565.918073	22.174835
85.572858	2560.475757	22.179853
85.498071	2579.472024	22.184871
85.818195	2586.037205	22.189888
85.936065	2593.809176	22.194906
86.243953	2594.992196	22.199923
86.276317	2588.469568	22.204941
86.223476	2579.957386	22.209959
86.647087	2591.434475	22.214976
86.913302	2608.077326	22.219994
87.142318	2601.024464	22.225011
86.876917	2604.067082	22.230029
87.023671	2606.352046	22.235047
87.347601	2599.338985	22.240064
87.347603	2599.429210	22.245082
87.576136	2592.311468	22.250099
87.376801	2587.113503	22.255117
87.316282	2591.190372	22.260135
87.676509	2591.698149	22.265152
87.701558	2600.566662	22.270170
87.677241	2608.797643	22.275187
87.756600	2593.746621	22.280205
87.417258	2607.232839	22.285223
87.690816	2595.527826	22.290240
87.532632	2597.831780	22.295258
87.639565	2594.426525	22.300275
87.796536	2599.571392	22.305293
87.794575	2623.208701	22.310311
87.983133	2624.511487	22.315328
87.693386	2625.049712	22.320346
88.135797	2638.509284	22.325363
88.160389	2651.578174	22.330381
88.234007	2654.476081	22.335399
88.411482	2660.131386	22.340416
88.573790	2666.759347	22.345434
88.665144	2654.266687	22.350451
88.713723	2669.587280	22.355469
88.928303	2677.393678	22.360487
89.312414	2678.080981	22.365504
89.202130	2687.544824	22.370522
89.403721	2688.239904	22.375539
89.887812	2677.946133	22.380557
89.785644	2678.143833	22.385575
89.814560	2680.515252	22.390592
89.686471	2680.277450	22.395610
90.005024	2676.156385	22.400627
90.051377	2683.207122	22.405645
89.658199	2677.465199	22.410663
89.965993	2664.127979	22.415680
89.878188	2681.796518	22.420698
89.937359	2675.326900	22.425715
90.319346	2672.536368	22.430733
89.781835	2682.300880	22.435751
90.188538	2684.006953	22.440768
89.983700	2699.422294	22.445786
90.260308	2698.411925	22.450803
90.381204	2714.521826	22.455821
90.458177	2731.953281	22.460839
90.970861	2728.258754	22.465856
90.896400	2730.811482	22.470874
90.857900	2729.751702	22.475891
91.217227	2723.981239	22.480909
90.989476	2728.658707	22.485927
91.464788	2740.443905	22.490944
91.662178	2748.466192	22.495962
91.692286	2748.553796	22.500979
92.001218	2745.778498	22.505997
92.040499	2752.540259	22.511015
92.548352	2746.126254	22.516032
91.830792	2753.414930	22.521050
92.272421	2750.692862	22.526067
92.205199	2753.918066	22.531085
92.351048	2750.881558	22.536103
92.248957	2745.857217	22.541120
92.045168	2742.294701	22.546138
92.525479	2742.205001	22.551155
92.701690	2740.534039	22.556173
92.438495	2744.527961	22.561191
92.750297	2734.695781	22.566208
92.897662	2761.578493	22.571226
92.631799	2761.958426	22.576243
92.937955	2771.208083	22.581261
92.890657	2771.356144	22.586279
92.931457	2769.120155	22.591296
93.122502	2763.791743	22.596314
92.893009	2788.170175	22.601331
93.255212	2790.805744	22.606349
92.764527	2804.405779	22.611367
93.408709	2798.764516	22.616384
93.450264	2821.378703	22.621402
93.714559	2824.520683	22.626419
94.077751	2819.121621	22.631437
93.980223	2826.161203	22.636455
94.038296	2811.787169	22.641472
94.118607	2818.582720	22.646490
94.198222	2824.359807	22.651507
94.355314	2836.189104	22.656525
94.492700	2851.878667	22.661543
94.932433	2839.758526	22.666560
94.634710	2852.842759	22.671578
94.669601	2840.899498	22.676595
95.088109	2842.439449	22.681613
95.063266	2850.349753	22.686631
94.927944	2839.693436	22.691648
95.089472	2836.668490	22.696666
95.087995	2844.262300	22.701683
95.548116	2843.518412	22.706701
95.162301	2845.897889	22.711719
95.457898	2862.699152	22.716736
95.890491	2876.073936	22.721754
95.677916	2874.014932	22.726771
95.788516	2868.570660	22.731789
95.763224	2876.684612	22.736807
95.938644	2869.994863	22.741824
95.683005	2869.072608	22.746842
95.993152	2871.006123	22.751859
96.237871	2881.964973	22.756877
96.005331	2888.943859	22.761895
96.410146	2890.661687	22.766912
96.388545	2896.211839	22.771930
96.284790	2890.196307	22.776947
96.726993	2902.411555	22.781965
96.551512	2917.511594	22.786983
96.990851	2916.842804	22.792000
96.917574	2921.106138	22.797018
97.099009	2926.675838	22.802035
97.189859	2911.763957	22.807053
97.058059	2918.735233	22.812071
97.358131	2931.631571	22.817088
97.287381	2937.328863	22.822106
97.535808	2939.164329	22.827123
97.748503	2935.011114	22.832141
97.937686	2937.297765	22.837159
98.302541	2933.219759	22.842176
98.059362	2930.956742	22.847194
97.957923	2934.507360	22.852211
98.098736	2934.324252	22.857229
98.462569	2955.401686	22.862247
98.408048	2959.634757	22.867264
98.761792	2954.531727	22.872282
98.510789	2955.508466	22.877299
98.787357	2960.162351	22.882317
99.071495	2954.782238	22.887335
98.832355	2945.439997	22.892352
99.124543	2954.498359	22.897370
99.101366	2957.333209	22.902387
99.525807	2964.093896	22.907405
99.426077	2979.727563	22.912423
99.659693	2980.722106	22.917440
99.422620	2982.919876	22.922458
99.711908	2984.890327	22.927475
99.766408	2980.558156	22.932493
99.742857	2976.782263	22.937511
99.807866	2975.826205	22.942528
100.013872	2976.548918	22.947546
99.685968	2975.539793	22.952563
100.077723	2990.041612	22.957581
100.249326	3005.570927	22.962599
100.376393	3004.047851	22.967616
100.775984	3006.520560	22.972634
100.326194	3011.236056	22.977651
100.410857	3002.829627	22.982669
100.458492	3011.131985	22.987687
100.647976	3019.665610	22.992704
101.215941	3032.898420	22.997722
100.882716	3029.420266	23.002739
101.178169	3022.691285	23.007757
100.868911	3031.544914	23.012775
100.748038	3042.688041	23.017792
101.392738	3052.258620	23.022810
100.888905	3064.053016	23.027827
101.601743	3057.306888	23.032845
102.086168	3073.034500	23.037863
102.503786	3069.412728	23.042880
102.384976	3059.406342	23.047898
102.699716	3050.253856	23.052915
102.696995	3039.477800	23.057933
102.739304	3047.078634	23.062951
102.952346	3042.728858	23.067968
102.895753	3041.007819	23.072986
102.858795	3047.018483	23.078003
102.657253	3042.743649	23.083021
103.194181	3043.362752	23.088039
102.869974	3041.366307	23.093056
103.156178	3034.301814	23.098074
102.893439	3039.334410	23.103091
103.028055	3034.194006	23.108109
103.116306	3054.005666	23.113127
103.164035	3061.369761	23.118144
103.015600	3066.902780	23.123162
103.053840	3062.008660	23.128179
103.335197	3077.281665	23.133197
103.592355	3085.359591	23.138215
103.704257	3090.390811	23.143232
103.838450	3096.257004	23.148250
103.626884	3098.556875	23.153267
104.455460	3118.226355	23.158285
104.534184	3109.252688	23.163303
104.528889	3114.817936	23.168320
104.716897	3121.607207	23.173338
104.540169	3113.703489	23.178355
104.680527	3112.145128	23.183373
104.922814	3119.471132	23.188391
105.087234	3120.212943	23.193408
105.210596	3128.297295	23.198426
105.218210	3146.680946	23.203443
105.403010	3138.713027	23.208461
105.364280	3143.899532	23.213479
105.121975	3141.890694	23.218496
105.488892	3137.104353	23.223514
105.208630	3148.905502	23.228531
105.727044	3164.986670	23.233549
105.825883	3167.961608	23.238567
105.852271	3165.077096	23.243584
106.069922	3166.510559	23.248602
106.223042	3191.232217	23.253619
106.493221	3185.967734	23.258637
106.800741	3187.447743	23.263655
106.435550	3195.861861	23.268672
106.632330	3184.577824	23.273690
106.485779	3194.907906	23.278707
106.792309	3187.997475	23.283725
106.985599	3198.591010	23.288743
107.057651	3210.732339	23.293760
107.497182	3209.654410	23.298778
107.341037	3212.189635	23.303795
107.487426	3214.735013	23.308813
107.854271	3215.010986	23.313831
107.690993	3209.213082	23.318848
107.889433	3209.931153	23.323866
107.519112	3213.992934	23.328883
107.774679	3207.105501	23.333901
107.701062	3227.985625	23.338919
108.224752	3241.030648	23.343936
108.406481	3233.893984	23.348954
108.285982	3240.954881	23.353971
108.554487	3246.684314	23.358989
108.890546	3241.613651	23.364007
108.553720	3239.102286	23.369024
108.732749	3232.866162	23.374042
108.797286	3247.305063	23.379059
108.944355	3245.312462	23.384077
109.147267	3252.016637	23.389095
108.983935	3257.623063	23.394112
109.491124	3241.924538	23.399130
109.293710	3260.411960	23.404147
109.451952	3250.901763	23.409165
109.756164	3255.488162	23.414183
109.696820	3280.260888	23.419200
110.059297	3275.998130	23.424218
109.930504	3278.397720	23.429235
110.077616	3277.936766	23.434253
110.329499	3268.342937	23.439271
110.062202	3286.008014	23.444288
110.203544	3277.701514	23.449306
110.065728	3292.335788	23.454323
110.382411	3302.590426	23.459341
110.632759	3298.036352	23.464359
110.476797	3309.220914	23.469376
110.808395	3307.723794	23.474394
111.118589	3321.114897	23.479411
110.979422	3326.151931	23.484429
111.509174	3318.542996	23.489447
111.387138	3320.273685	23.494464
111.703500	3312.675671	23.499482
111.751572	3324.309192	23.504499
111.816031	3334.880051	23.509517
112.031344	3337.792819	23.514535
112.095571	3348.714945	23.519552
112.196344	3347.330850	23.524570
112.157941	3349.306779	23.529587
112.638265	3344.020838	23.534605
112.963011	3341.747205	23.539623
112.681219	3345.000180	23.544640
112.731676	3333.402429	23.549658
112.676436	3343.980906	23.554675
112.561675	3340.588964	23.559693
113.064300	3355.108994	23.564711
112.976704	3369.412942	23.569728
113.130777	3364.949205	23.574746
112.867113	3371.040840	23.579763
113.343696	3383.070440	23.584781
113.226521	3390.352532	23.589799
113.552064	3401.867722	23.594816
113.821323	3399.928108	23.599834
113.875340	3398.248171	23.604851
113.951806	3395.891607	23.609869
114.611544	3410.986532	23.614887
114.469890	3425.210495	23.619904
114.592319	3423.394017	23.624922
114.742636	3426.377807	23.629939
114.580160	3424.299409	23.634957
114.947580	3418.942362	23.639975
114.882558	3417.864482	23.644992
115.012842	3410.847292	23.650010
115.178000	3416.387576	23.655027
115.037788	3413.432559	23.660045
115.562831	3422.228995	23.665063
115.023004	3426.928413	23.670080
115.496773	3434.139067	23.675098
115.379157	3442.885205	23.680115
115.620986	3441.837632	23.685133
115.531613	3437.458675	23.690151
115.488780	3461.458785	23.695168
115.559794	3464.971127	23.700186
116.318943	3465.191211	23.705203
116.256031	3473.834991	23.710221
116.464402	3470.846663	23.715239
116.401908	3481.567789	23.720256
116.564710	3491.318439	23.725274
116.398320	3495.486702	23.730291
116.688428	3498.173312	23.735309
116.806497	3492.279502	23.740327
116.760379	3494.139390	23.745344
117.218248	3506.626570	23.750362
117.617305	3515.551017	23.755379
117.373134	3528.146178	23.760397
117.612206	3514.212848	23.765415
117.861874	3516.127323	23.770432
117.748121	3515.828070	23.775450
118.089020	3517.487254	23.780467
118.001274	3522.923761	23.785485
118.149577	3523.540686	23.790503
118.028499	3537.847969	23.795520
118.069147	3537.764127	23.800538
118.528188	3544.014948	23.805555
118.842384	3549.768823	23.810573
118.811922	3536.360866	23.815591
118.787481	3555.780746	23.820608
118.894634	3570.097128	23.825626
119.039066	3573.070107	23.830643
119.286654	3570.323723	23.835661
119.498501	3567.337951	23.840679
119.258395	3569.781215	23.845696
119.622818	3577.913695	23.850714
119.918367	3591.027105	23.855731
119.928420	3593.116711	23.860749
120.576869	3586.590497	23.865767
120.453931	3592.229336	23.870784
120.154871	3590.842117	23.875802
120.659153	3596.505869	23.880819
120.384394	3595.304808	23.885837
120.285451	3590.428904	23.890855
120.442529	3600.881052	23.895872
120.392643	3615.468388	23.900890
121.094498	3610.334288	23.905907
120.131741	3627.021839	23.910925
121.003080	3619.510557	23.915943
120.953055	3642.602178	23.920960
121.609522	3636.056110	23.925978
121.655105	3632.963584	23.930995
121.894966	3629.008865	23.936013
121.793973	3637.764960	23.941031
121.669639	3638.977887	23.946048
121.711187	3659.703675	23.951066
122.025436	3664.746861	23.956083
122.029078	3665.384987	23.961101
122.190214	3658.207440	23.966119
122.577797	3674.006427	23.971136
122.470527	3694.506868	23.976154
122.598014	3691.575596	23.981171
122.632534	3696.311909	23.986189
122.850593	3692.055232	23.991207
122.558886	3708.710912	23.996224
123.034877	3717.692039	24.001242
123.384327	3721.884815	24.006259
123.312474	3722.698062	24.011277
123.389820	3732.093276	24.016295
123.715617	3742.934965	24.021312
123.675860	3748.871942	24.026330
124.290928	3742.379542	24.031347
124.151433	3750.769189	24.036365
124.356860	3742.684148	24.041383
124.188326	3751.047102	24.046400
124.472253	3741.903648	24.051418
124.783395	3760.596477	24.056435
124.764041	3775.179694	24.061453
125.032981	3770.719663	24.066471
125.008918	3774.413587	24.071488
125.075191	3768.206945	24.076506
125.275177	3765.177030	24.081523
125.580261	3772.314575	24.086541
125.272150	3765.165450	24.091559
125.385164	3773.000634	24.096576
125.576684	3779.291118	24.101594
125.943097	3788.097488	24.106611
125.498439	3794.826028	24.111629
125.696137	3792.871045	24.116647
125.979510	3794.142091	24.121664
125.917853	3816.991372	24.126682
126.394243	3812.460758	24.131699
126.346931	3828.250396	24.136717
126.408917	3822.637046	24.141735
126.473482	3838.160892	24.146752
126.567433	3853.186905	24.151770
126.524589	3854.548979	24.156787
127.036319	3859.007092	24.161805
127.140467	3867.995531	24.166823
127.357421	3881.054865	24.171840
127.170488	3885.225844	24.176858
127.734980	3877.699092	24.181875
127.234727	3904.209821	24.186893
127.873676	3898.879716	24.191911
127.732497	3907.583156	24.196928
128.304902	3913.432626	24.201946
128.597363	3922.794309	24.206963
128.813757	3936.227458	24.211981
129.108531	3925.814985	24.216999
129.102059	3923.750461	24.222016
129.087289	3925.804452	24.227034
129.351853	3923.839958	24.232051
128.881802	3918.619427	24.237069
129.355481	3924.432483	24.242087
129.553712	3916.731672	24.247104
129.250531	3919.649279	24.252122
129.533000	3938.091912	24.257139
129.527389	3951.153108	24.262157
129.404225	3954.254335	24.267175
129.979804	3958.014009	24.272192
129.915515	3974.001121	24.277210
130.078067	3976.493548	24.282227
130.337608	3984.373880	24.287245
130.684857	3975.175706	24.292263
130.424817	3989.773770	24.297280
130.540593	3997.098296	24.302298
130.950887	3995.586116	24.307315
130.903089	4006.846195	24.312333
131.315772	4004.587836	24.317351
131.559562	4030.274305	24.322368
131.522390	4034.684349	24.327386
131.691462	4044.529597	24.332403
131.867966	4043.431768	24.337421
132.211073	4044.502759	24.342439
132.060763	4039.278865	24.347456
132.156792	4045.417523	24.352474
132.268293	4026.999439	24.357491
132.040666	4042.093050	24.362509
132.340144	4048.650064	24.367527
132.453107	4056.251504	24.372544
132.436218	4061.036997	24.377562
132.856533	4070.032665	24.382579
132.735154	4085.418224	24.387597
133.226005	4087.402700	24.392615
133.286690	4080.734189	24.397632
133.295702	4081.052495	24.402650
133.400584	4081.436831	24.407667
133.612876	4092.798815	24.412685
133.546156	4102.894982	24.417703
134.091168	4103.061546	24.422720
133.938905	4104.463413	24.427738
133.945664	4110.746818	24.432755
133.964674	4130.691009	24.437773
134.494307	4137.729725	24.442791
134.521103	4139.497289	24.447808
134.219884	4148.999924	24.452826
134.740554	4148.083729	24.457843
134.748428	4161.611447	24.462861
134.893453	4167.854658	24.467879
135.002721	4166.541144	24.472896
135.324877	4187.559023	24.477914
135.659107	4185.020667	24.482931
135.591828	4193.252900	24.487949
135.816136	4188.486704	24.492967
135.890604	4179.120940	24.497984
136.178333	4196.790441	24.503002
136.353773	4206.564647	24.508019
136.698335	4205.922528	24.513037
136.984836	4209.660821	24.518055
137.165361	4205.670500	24.523072
136.458574	4207.356341	24.528090
136.962713	4200.390702	24.533107
137.057003	4206.297389	24.538125
137.338857	4225.852459	24.543143
137.619906	4233.386780	24.548160
137.371269	4240.741038	24.553178
137.689449	4232.854832	24.558195
137.795761	4240.009357	24.563213
137.711824	4242.849773	24.568231
137.666851	4249.826952	24.573248
137.692173	4257.817078	24.578266
138.162068	4261.264348	24.583283
138.344622	4283.394628	24.588301
138.239848	4285.581697	24.593319
138.305789	4286.266236	24.598336
138.398943	4304.585500	24.603354
138.842309	4314.092542	24.608371
138.833681	4328.376021	24.613389
139.041425	4324.145690	24.618407
139.056524	4340.605155	24.623424
139.554349	4352.950156	24.628442
139.532546	4357.044305	24.633459
139.644748	4355.436538	24.638477
139.777010	4377.355553	24.643495
140.018855	4377.135229	24.648512
140.128615	4387.522890	24.653530
140.420700	4378.344640	24.658547
140.505550	4388.508039	24.663565
140.559818	4403.849078	24.668583
140.684475	4400.122333	24.673600
140.646287	4411.173987	24.678618
140.874538	4419.588160	24.683635
141.258675	4434.774599	24.688653
141.245056	4440.347208	24.693671
141.601278	4436.252925	24.698688
141.641427	4436.773206	24.703706
141.688679	4452.376131	24.708723
141.986064	4456.547407	24.713741
142.225683	4464.170603	24.718759
142.331936	4455.946077	24.723776
142.319593	4456.395508	24.728794
142.601149	4464.291340	24.733811
142.644124	4450.001389	24.738829
142.705432	4469.513734	24.743847
143.020137	4480.627506	24.748864
143.089509	4491.114065	24.753882
143.181073	4476.748316	24.758899
143.282774	4482.919284	24.763917
143.451502	4488.995677	24.768935
143.791833	4485.693132	24.773952
143.721691	4508.468826	24.778970
144.159675	4511.155940	24.783987
143.842763	4516.651206	24.789005
143.719411	4512.522893	24.794023
144.157252	4518.298792	24.799040
144.109882	4530.978334	24.804058
144.018677	4541.316676	24.809075
144.434348	4543.672782	24.814093
144.452594	4563.342006	24.819111
144.694497	4578.041013	24.824128
144.630722	4580.318990	24.829146
145.168351	4592.203962	24.834163
145.593567	4588.877105	24.839181
145.391937	4595.505499	24.844199
145.729585	4606.483254	24.849216
145.528490	4627.615128	24.854234
146.378142	4623.650170	24.859251
146.361472	4623.794752	24.864269
146.437129	4621.250308	24.869287
146.484979	4623.505874	24.874304
146.608960	4649.365977	24.879322
146.712987	4647.388596	24.884339
146.972227	4655.127558	24.889357
147.065248	4659.138197	24.894375
147.102891	4671.594289	24.899392
147.635657	4676.342523	24.904410
147.651512	4679.056238	24.909427
148.088508	4673.524621	24.914445
147.654083	4677.422548	24.919463
147.550363	4685.022364	24.924480
148.018334	4699.883309	24.929498
148.124875	4701.436907	24.934515
148.333401	4703.218552	24.939533
148.349084	4727.252256	24.944551
149.113801	4729.792385	24.949568
149.118019	4742.479308	24.954586
149.091087	4739.028024	24.959603
149.370069	4731.058279	24.964621
149.165842	4745.283161	24.969639
149.669351	4756.081564	24.974656
149.222077	4763.965112	24.979674
149.731463	4756.765245	24.984691
149.955479	4765.552822	24.989709
149.678417	4794.569155	24.994727
150.441594	4789.241030	24.999744
150.217244	4795.504691	25.004762
150.179542	4797.523213	25.009779
150.738141	4803.348531	25.014797
150.594899	4817.861081	25.019815
150.906993	4817.638573	25.024832
151.018847	4818.484073	25.029850
151.245828	4842.564878	25.034867
151.596210	4845.435881	25.039885
151.553195	4846.249530	25.044903
151.766416	4849.538598	25.049920
151.515660	4857.997658	25.054938
151.358342	4877.882993	25.059955
151.433535	4884.021492	25.064973
151.746335	4901.876652	25.069991
151.987963	4906.637717	25.075008
152.356641	4912.261398	25.080026
152.366131	4925.416986	25.085043
152.702997	4929.785045	25.090061
152.669325	4934.630286	25.095079
153.044111	4950.785908	25.100096
152.926637	4972.200525	25.105114
152.894235	4968.740645	25.110131
153.319736	4988.464263	25.115149
153.075693	4993.608974	25.120167
153.579192	4996.782285	25.125184
153.944373	5020.952318	25.130202
154.174861	5020.898470	25.135219
154.498037	5016.499206	25.140237
154.343702	5041.274289	25.145255
154.430354	5050.474615	25.150272
154.883230	5054.094210	25.155290
154.929811	5053.330490	25.160307
155.570488	5072.983938	25.165325
155.394816	5081.106992	25.170343
155.726280	5069.897755	25.175360
155.684310	5087.952837	25.180378
155.501387	5079.938889	25.185395
155.882163	5082.081122	25.190413
156.243668	5101.299615	25.195431
156.208028	5109.763361	25.200448
156.316074	5105.854121	25.205466
156.442033	5131.761943	25.210483
156.733121	5128.443792	25.215501
156.730478	5145.304762	25.220519
157.041443	5135.162892	25.225536
157.050786	5153.010296	25.230554
157.121476	5160.072690	25.235571
157.659905	5167.137196	25.240589
157.147802	5173.021776	25.245607
157.594490	5189.857235	25.250624
157.793337	5192.601387	25.255642
157.839628	5226.899266	25.260659
158.427430	5223.298849	25.265677
158.063855	5237.710434	25.270695
158.672327	5242.360463	25.275712
158.417349	5260.392725	25.280730
158.746359	5262.801882	25.285747
159.102330	5270.790551	25.290765
159.050088	5291.484399	25.295783
159.100113	5291.248568	25.300800
159.734447	5295.648604	25.305818
159.710604	5320.220588	25.310835
159.916444	5318.117582	25.315853
159.978198	5329.466793	25.320871
159.813306	5331.938826	25.325888
160.401604	5351.849385	25.330906
159.894245	5358.349141	25.335923
160.863698	5375.285699	25.340941
160.572679	5390.642333	25.345959
161.043781	5397.145512	25.350976
161.168003	5395.057583	25.355994
161.011654	5404.368441	25.361011
161.373931	5409.510569	25.366029
161.171337	5431.132071	25.371047
161.385356	5440.889632	25.376064
162.006133	5453.718420	25.381082
161.952850	5465.618399	25.386099
161.868869	5466.752325	25.391117
161.861365	5483.322262	25.396135
162.414817	5504.506024	25.401152
162.794616	5510.706177	25.406170
162.637931	5509.672861	25.411187
162.853742	5511.932252	25.416205
162.931878	5535.797753	25.421223
163.231734	5532.135463	25.426240
163.506214	5534.373330	25.431258
163.566417	5559.721733	25.436275
163.733534	5564.922212	25.441293
164.151154	5571.101163	25.446311
164.138986	5562.189190	25.451328
164.353908	5582.072855	25.456346
164.749240	5592.347088	25.461363
164.773130	5585.282357	25.466381
164.830698	5588.777711	25.471399
165.034404	5610.818144	25.476416
165.137934	5614.557927	25.481434
164.789104	5623.678676	25.486451
165.187570	5625.217905	25.491469
165.333572	5648.531258	25.496487
165.598996	5660.985864	25.501504
166.008709	5666.708564	25.506522
165.951742	5692.006479	25.511539
166.414892	5682.181674	25.516557
166.492864	5700.395598	25.521575
166.504830	5715.863845	25.526592
166.830966	5709.090055	25.531610
166.755827	5725.224083	25.536627
166.727045	5736.537380	25.541645
167.339632	5749.521350	25.546663
167.533467	5764.983165	25.551680
167.616274	5769.169839	25.556698
167.560106	5781.609258	25.561715
167.948145	5793.691608	25.566733
168.019719	5798.783539	25.571751
168.057888	5807.102333	25.576768
168.568755	5819.124987	25.581786
168.608661	5837.576141	25.586803
168.947467	5834.108175	25.591821
169.267858	5839.078591	25.596839
169.152472	5861.622715	25.601856
169.507982	5878.640193	25.606874
169.705195	5877.021350	25.611891
170.140029	5872.939678	25.616909
169.779095	5881.237158	25.621927
169.627395	5887.001687	25.626944
170.377152	5889.700439	25.631962
170.267113	5907.173863	25.636979
170.396105	5916.696121	25.641997
170.649918	5927.130260	25.647015
170.621924	5946.981351	25.652032
170.837135	5944.581355	25.657050
170.877920	5967.924412	25.662067
171.349449	5981.166637	25.667085
171.467267	5990.389131	25.672103
171.817930	6003.589162	25.677120
171.789033	6005.342528	25.682138
171.846459	6021.662055	25.687156
172.130620	6021.540250	25.692173
172.092029	6035.268659	25.697191
172.313112	6051.737551	25.702208
172.852009	6071.253936	25.707226
172.900380	6081.507954	25.712244
173.265562	6083.404809	25.717261
173.311888	6094.843762	25.722279
173.304687	6106.486128	25.727296
173.594483	6106.605979	25.732314
173.830335	6122.081666	25.737332
173.774145	6126.573417	25.742349
174.135563	6149.654153	25.747367
174.128129	6139.311525	25.752384
174.270936	6154.713646	25.757402
174.244715	6174.909710	25.762420
174.824021	6171.505037	25.767437
175.124436	6180.111416	25.772455
175.034490	6192.029037	25.777472
175.525560	6198.339426	25.782490
175.361131	6198.810146	25.787508
175.782099	6220.864295	25.792525
175.813515	6226.651403	25.797543
175.624090	6236.752706	25.802560
176.279023	6237.802952	25.807578
176.384929	6263.004716	25.812596
176.656963	6259.886396	25.817613
176.745013	6257.573566	25.822631
176.760214	6285.376972	25.827648
177.045661	6286.349766	25.832666
176.883237	6290.800865	25.837684
177.489748	6309.538408	25.842701
177.538905	6313.337767	25.847719
177.488701	6329.183156	25.852736
178.013370	6338.370005	25.857754
177.679488	6358.788942	25.862772
178.154472	6371.294481	25.867789
178.409612	6377.821219	25.872807
178.528568	6391.550634	25.877824
178.978683	6402.963919	25.882842
178.593137	6411.346088	25.887860
179.456726	6415.880199	25.892877
179.264238	6423.753890	25.897895
179.361004	6440.308354	25.902912
179.776618	6444.322753	25.907930
179.832073	6456.611898	25.912948
180.249409	6466.795632	25.917965
180.497464	6471.296186	25.922983
180.551860	6502.743428	25.928000
181.063838	6496.070076	25.933018
181.215263	6502.412399	25.938036
181.137496	6499.063663	25.943053
181.414170	6515.255248	25.948071
181.401089	6527.031221	25.953088
181.465469	6526.596084	25.958106
181.753619	6544.391024	25.963124
181.863386	6559.919519	25.968141
182.138474	6567.188149	25.973159
182.063786	6578.000824	25.978176
182.712127	6576.152849	25.983194
182.861876	6595.569688	25.988212
182.660206	6619.743856	25.993229
182.988105	6624.547872	25.998247
183.103438	6638.824731	26.003264
183.264700	6640.957841	26.008282
183.457653	6662.732931	26.013300
183.507790	6673.826678	26.018317
183.901761	6686.553820	26.023335
183.806013	6697.042399	26.028352
184.208221	6708.461474	26.033370
184.514969	6722.178203	26.038388
184.771851	6723.529104	26.043405
184.745378	6733.733709	26.048423
184.587926	6749.628779	26.053440
185.083510	6759.674510	26.058458
185.313616	6781.967406	26.063476
185.078665	6783.797502	26.068493
185.468421	6800.523596	26.073511
185.748656	6819.470140	26.078528
186.215760	6829.429262	26.083546
186.137219	6843.365049	26.088564
186.567663	6853.021491	26.093581
186.680762	6860.952718	26.098599
187.062156	6875.833204	26.103616
187.131436	6870.850060	26.108634
187.160142	6883.299922	26.113652
187.270521	6904.450217	26.118669
187.677495	6901.479570	26.123687
187.511918	6912.127931	26.128704
188.084905	6917.888649	26.133722
188.201128	6930.664331	26.138740
188.241758	6941.325835	26.143757
188.195601	6944.172293	26.148775
188.333592	6963.381220	26.153792
188.604910	6976.855919	26.158810
188.943039	6986.604918	26.163828
189.025559	7011.987393	26.168845
189.530665	7023.425107	26.173863
189.344486	7036.881861	26.178880
189.839708	7045.265059	26.183898
190.045055	7056.570469	26.188916
189.867849	7067.602093	26.193933
190.336169	7092.011852	26.198951
190.449845	7096.362330	26.203968
190.810814	7116.191450	26.208986
191.096701	7122.759092	26.214004
191.067059	7127.550774	26.219021
191.325795	7147.650490	26.224039
191.756164	7156.481644	26.229056
191.813389	7166.574998	26.234074
191.887494	7190.190024	26.239092
191.713822	7196.023252	26.244109
192.103374	7209.570734	26.249127
192.419826	7224.726960	26.254144
192.852903	7243.344663	26.259162
193.230683	7254.944619	26.264180
193.163496	7261.089494	26.269197
193.524935	7274.631446	26.274215
193.752199	7286.726590	26.279232
194.023227	7290.602092	26.284250
194.104133	7292.903767	26.289268
194.272320	7311.688281	26.294285
194.422496	7318.347787	26.299303
194.581068	7333.032435	26.304320
194.678893	7350.710127	26.309338
194.967214	7367.324431	26.314356
194.895696	7372.209764	26.319373
195.053186	7378.000838	26.324391
195.210879	7380.133852	26.329408
195.227402	7402.110091	26.334426
195.917777	7414.528813	26.339444
196.095281	7443.617305	26.344461
196.251318	7438.844902	26.349479
196.537064	7453.620461	26.354496
196.826282	7477.179034	26.359514
197.432647	7472.791297	26.364532
196.988400	7480.681979	26.369549
197.305057	7494.264616	26.374567
197.574956	7500.019010	26.379584
197.681237	7516.538362	26.384602
197.867156	7521.549690	26.389620
197.662343	7545.672219	26.394637
198.307835	7557.489593	26.399655
198.530138	7576.155182	26.404672
198.383756	7579.567372	26.409690
199.031434	7591.269406	26.414708
198.941698	7599.339344	26.419725
199.146136	7599.113364	26.424743
199.417842	7618.731819	26.429760
199.450229	7629.598375	26.434778
199.605626	7628.673945	26.439796
199.698157	7650.069222	26.444813
199.909450	7663.397689	26.449831
200.217010	7684.708578	26.454848
200.303536	7697.808025	26.459866
200.699655	7705.746386	26.464884
200.497017	7734.069673	26.469901
201.143164	7735.975360	26.474919
200.948314	7753.773632	26.479936
201.539065	7763.809763	26.484954
201.849104	7775.464638	26.489972
201.974109	7800.483717	26.494989
202.295529	7800.002056	26.500007
202.460537	7804.467902	26.505024
202.566856	7823.488546	26.510042
202.609162	7824.753759	26.515060
202.900062	7856.153495	26.520077
202.843256	7857.894354	26.525095
203.349880	7871.404904	26.530112
203.706103	7883.947844	26.535130
203.860698	7877.222018	26.540148
203.848109	7899.740983	26.545165
203.964902	7919.810032	26.550183
204.325961	7935.559004	26.555200
204.588619	7953.419611	26.560218
204.815122	7959.831223	26.565236
204.713119	7986.163488	26.570253
205.096773	7985.873964	26.575271
205.465531	8006.719064	26.580288
205.480429	8016.159066	26.585306
206.112408	8034.932248	26.590324
206.317647	8039.731008	26.595341
206.398445	8045.077356	26.600359
206.796075	8060.643161	26.605376
206.828287	8075.288757	26.610394
207.131119	8072.663619	26.615412
206.908009	8088.265253	26.620429
207.302860	8108.841492	26.625447
207.410564	8120.023608	26.630464
207.635876	8146.917167	26.635482
208.170997	8140.734788	26.640500
208.046178	8160.777968	26.645517
208.428920	8176.565339	26.650535
208.573047	8182.195072	26.655552
208.666611	8203.311277	26.660570
209.403540	8204.010949	26.665588
209.278604	8222.794646	26.670605
209.287692	8238.643934	26.675623
209.514176	8245.411720	26.680640
209.586778	8271.318532	26.685658
210.064915	8268.494193	26.690676
210.299815	8300.337327	26.695693
210.209073	8304.496684	26.700711
210.435539	8314.806947	26.705728
210.756380	8328.793712	26.710746
211.197696	8341.385946	26.715764
211.249532	8366.996223	26.720781
211.593423	8366.491135	26.725799
211.597116	8379.022715	26.730816
211.589956	8391.720739	26.735834
212.429445	8411.647138	26.740852
212.492333	8419.076999	26.745869
212.855660	8425.513414	26.750887
213.092131	8436.948569	26.755904
213.176208	8448.983224	26.760922
213.391246	8451.557479	26.765940
213.228775	8475.177333	26.770957
213.792206	8487.414676	26.775975
213.807311	8483.613737	26.780992
213.986635	8492.261115	26.786010
214.283997	8502.411667	26.791028
214.503980	8507.390097	26.796045
214.746724	8525.125450	26.801063
215.032240	8535.510370	26.806080
215.198205	8539.024666	26.811098
215.622000	8549.453662	26.816116
215.571130	8567.889923	26.821133
215.880477	8573.611394	26.826151
216.110448	8576.227311	26.831168
216.378755	8602.796270	26.836186
216.623282	8596.286067	26.841204
216.840268	8612.833129	26.846221
216.689712	8619.991982	26.851239
217.057988	8629.319493	26.856256
217.280862	8645.564694	26.861274
217.609963	8661.900248	26.866292
217.597530	8670.298238	26.871309
217.878982	8683.975159	26.876327
218.128691	8693.718576	26.881344
218.085698	8710.592368	26.886362
218.559643	8710.487190	26.891380
219.050258	8730.771878	26.896397
219.266879	8754.419981	26.901415
219.535706	8761.853722	26.906432
219.385599	8776.309569	26.911450
219.981256	8780.929699	26.916468
220.287856	8790.347078	26.921485
220.412285	8796.790106	26.926503
220.716418	8806.914523	26.931520
220.554887	8821.121006	26.936538
221.056061	8824.457773	26.941556
221.419645	8846.974094	26.946573
221.274055	8845.007583	26.951591
221.592995	8854.565543	26.956608
221.731720	8870.152941	26.961626
221.556162	8864.752805	26.966644
221.709660	8896.103282	26.971661
221.862504	8918.230772	26.976679
222.582794	8924.758762	26.981696
222.773559	8943.698225	26.986714
223.278002	8964.118780	26.991732
223.370393	8969.948783	26.996749
223.806624	8985.669807	27.001767
223.974030	8987.492626	27.006784
224.110528	9002.627555	27.011802
224.263641	9015.572898	27.016820
224.690456	9029.601819	27.021837
224.692177	9032.196513	27.026855
225.174042	9037.834450	27.031872
225.053482	9063.857237	27.036890
225.203481	9070.827889	27.041908
225.298754	9092.723304	27.046925
225.491254	9109.038601	27.051943
225.716899	9114.718979	27.056960
225.968406	9137.078588	27.061978
226.021249	9146.011162	27.066996
226.650764	9167.521249	27.072013
226.266644	9188.898230	27.077031
226.629846	9203.392382	27.082048
226.827821	9222.908424	27.087066
227.068453	9241.635949	27.092084
227.480004	9266.195514	27.097101
227.305182	9296.379272	27.102119
228.051179	9315.228838	27.107136
227.991404	9336.299444	27.112154
228.739367	9333.021397	27.117172
229.495993	9347.586840	27.122189
229.109738	9355.430233	27.127207
229.789087	9361.468090	27.132224
229.815948	9373.216703	27.137242
229.904090	9372.400995	27.142260
230.205739	9374.664855	27.147277
230.374697	9382.125659	27.152295
230.530020	9392.689458	27.157312
230.490156	9409.129395	27.162330
230.890674	9425.677641	27.167348
231.454186	9437.246082	27.172365
231.118750	9448.849111	27.177383
231.674170	9458.152431	27.182400
231.833045	9469.720916	27.187418
231.908401	9496.261850	27.192436
232.242029	9509.295092	27.197453
232.124215	9528.756641	27.202471
232.524684	9537.243504	27.207488
232.568195	9563.351019	27.212506
232.742803	9578.059499	27.217524
233.285400	9597.064390	27.222541
233.403986	9619.718465	27.227559
233.837096	9632.227996	27.232576
234.102414	9652.037503	27.237594
234.227911	9665.498438	27.242612
234.461414	9678.126129	27.247629
234.790431	9699.750489	27.252647
235.153423	9713.155606	27.257664
235.244888	9727.102787	27.262682
235.710920	9735.708891	27.267700
235.787111	9760.189225	27.272717
236.019006	9771.904189	27.277735
236.492510	9781.163749	27.282752
236.482284	9800.741743	27.287770
236.825113	9822.515242	27.292788
237.069886	9828.767021	27.297805
237.210280	9849.669661	27.302823
237.636319	9857.264600	27.307840
237.563099	9876.514355	27.312858
237.717293	9893.428438	27.317876
238.224915	9900.804274	27.322893
238.005258	9928.990080	27.327911
238.584477	9931.802085	27.332928
238.745458	9947.054388	27.337946
239.009019	9965.867987	27.342964
239.254495	9974.092399	27.347981
239.117883	10004.789544	27.352999
239.781012	10011.043045	27.358016
239.981549	10030.852714	27.363034
240.383688	10047.373760	27.368052
240.669933	10065.343116	27.373069
240.751073	10095.419036	27.378087
241.144087	10102.624860	27.383104
240.976640	10115.231030	27.388122
241.582203	10131.936717	27.393140
241.822207	10155.801242	27.398157
241.818902	10171.437838	27.403175
242.319089	10188.182298	27.408192
242.336612	10214.083244	27.413210
242.868106	10220.109665	27.418228
243.113735	10232.262301	27.423245
243.451587	10243.080851	27.428263
243.780052	10262.537165	27.433280
244.085433	10278.019559	27.438298
244.422865	10277.346893	27.443316
244.395065	10294.977726	27.448333
244.542557	10311.522289	27.453351
244.827818	10310.560457	27.458368
245.087247	10330.062944	27.463386
245.183604	10339.799660	27.468404
245.515413	10344.776699	27.473421
245.465262	10370.573287	27.478439
246.095460	10378.393090	27.483456
245.944445	10400.734426	27.488474
246.201099	10405.767256	27.493492
246.297324	10431.509773	27.498509
246.447347	10446.615461	27.503527
246.702560	10458.781651	27.508544
246.670327	10483.767129	27.513562
247.034662	10516.569372	27.518580
247.574839	10532.769475	27.523597
247.565881	10551.064773	27.528615
247.882467	10573.046895	27.533632
248.527371	10597.071950	27.538650
248.497427	10614.598703	27.543668
249.092179	10639.905287	27.548685
249.205035	10654.020692	27.553703
249.474139	10663.824338	27.558720
250.060797	10682.563232	27.563738
250.191038	10697.317109	27.568756
250.783140	10703.821362	27.573773
250.753474	10726.034338	27.578791
250.987512	10734.217702	27.583808
251.105154	10755.609025	27.588826
251.559827	10765.850002	27.593844
251.805589	10779.258082	27.598861
251.599888	10809.421420	27.603879
252.171540	10815.309848	27.608896
252.187383	10826.997528	27.613914
252.357127	10846.872387	27.618932
253.067718	10862.710562	27.623949
253.030728	10891.552459	27.628967
253.314931	10899.719724	27.633984
253.480969	10919.146204	27.639002
253.620677	10938.077560	27.644020
253.844812	10951.851781	27.649037
254.217240	10986.145855	27.654055
254.427124	10993.257124	27.659072
254.777410	11023.905546	27.664090
255.088534	11047.321564	27.669108
255.622934	11052.360620	27.674125
255.778399	11075.517237	27.679143
256.021677	11088.708534	27.684160
256.317457	11112.547910	27.689178
256.638672	11128.501226	27.694196
257.126468	11129.288779	27.699213
257.294643	11156.018776	27.704231
257.532937	11167.824304	27.709248
257.940085	11169.800720	27.714266
258.036884	11198.515442	27.719284
258.656632	11198.616189	27.724301
258.495360	11209.821344	27.729319
258.321298	11227.635768	27.734336
258.512474	11242.028662	27.739354
258.633040	11259.958230	27.744372
258.962638	11277.744490	27.749389
259.393948	11301.386801	27.754407
260.184340	11324.235401	27.759424
260.425376	11340.993233	27.764442
260.323678	11362.030876	27.769460
260.358479	11367.346551	27.774477
261.000026	11392.061960	27.779495
261.120241	11401.586578	27.784512
261.907461	11417.281827	27.789530
262.091659	11422.137877	27.794548
262.030622	11430.417712	27.799565
262.229134	11445.994557	27.804583
262.681058	11446.877886	27.809600
262.588912	11467.011163	27.814618
262.914536	11487.957750	27.819636
262.894711	11503.082299	27.824653
263.342557	11517.012218	27.829671
263.806811	11535.298056	27.834688
263.828975	11556.728305	27.839706
264.030806	11576.061405	27.844724
264.582791	11586.907659	27.849741
264.422073	11613.870919	27.854759
264.901273	11626.918026	27.859776
265.243597	11642.365677	27.864794
265.141694	11669.297231	27.869812
265.431901	11687.876786	27.874829
265.999131	11703.731643	27.879847
265.738527	11729.088551	27.884864
266.322175	11743.858152	27.889882
266.731908	11774.518642	27.894900
266.851281	11785.803804	27.899917
267.054324	11811.607262	27.904935
267.385829	11829.084954	27.909952
267.747881	11851.849199	27.914970
267.783551	11879.160162	27.919988
268.336371	11897.382900	27.925005
268.533232	11918.346630	27.930023
268.927395	11944.668628	27.935040
269.484509	11958.626540	27.940058
269.580358	11985.281631	27.945076
269.613202	11989.255227	27.950093
269.970597	12006.309654	27.955111
270.306913	12031.675383	27.960128
270.894963	12044.588199	27.965146
270.702571	12078.341443	27.970164
271.250033	12078.195732	27.975181
271.531579	12099.059007	27.980199
272.102848	12112.817730	27.985216
272.498365	12134.385497	27.990234
272.327999	12152.485549	27.995252
272.798342	12162.543601	28.000269
272.839716	12179.299106	28.005287
273.241578	12208.499333	28.010304
273.508895	12218.357799	28.015322
273.898554	12235.555257	28.020340
274.050153	12245.759097	28.025357
274.424544	12274.278492	28.030375
274.622214	12282.692434	28.035392
275.131482	12301.319953	28.040410
275.165960	12326.129399	28.045428
275.603949	12341.153734	28.050445
275.443874	12356.111612	28.055463
275.916294	12374.371835	28.060480
276.321322	12394.475968	28.065498
276.390500	12418.759775	28.070516
276.466505	12430.624605	28.075533
276.657496	12447.406049	28.080551
276.863479	12476.758948	28.085568
277.308215	12491.787033	28.090586
277.614093	12513.798781	28.095604
277.624290	12527.181117	28.100621
278.183407	12547.570384	28.105639
278.238320	12587.401331	28.110656
279.202236	12607.885985	28.115674
279.119565	12627.380895	28.120692
279.340116	12649.993183	28.125709
279.683802	12667.575347	28.130727
279.795580	12691.501084	28.135744
280.331905	12704.922551	28.140762
280.636913	12724.269882	28.145780
281.169204	12743.806546	28.150797
281.368507	12755.666964	28.155815
281.271887	12768.833945	28.160832
281.699872	12783.395454	28.165850
281.794703	12797.555108	28.170868
282.109302	12817.224025	28.175885
282.441942	12830.156108	28.180903
282.742529	12852.695545	28.185920
283.311788	12870.198042	28.190938
283.645634	12899.349308	28.195956
283.815439	12896.033899	28.200973
283.703497	12918.521942	28.205991
284.239031	12943.380192	28.211008
284.728921	12956.765428	28.216026
284.700568	12979.698312	28.221044
285.351806	12998.820038	28.226061
285.336639	13015.188628	28.231079
285.120387	13034.614730	28.236096
285.628726	13048.632089	28.241114
286.038637	13079.578682	28.246132
286.379887	13103.427642	28.251149
286.644520	13123.930991	28.256167
286.645945	13150.286856	28.261184
287.303510	13163.825742	28.266202
287.529684	13188.953054	28.271220
287.762492	13217.762299	28.276237
288.070433	13232.208549	28.281255
288.183892	13258.546044	28.286272
288.878074	13282.719805	28.291290
288.849631	13304.033078	28.296308
289.278907	13324.652839	28.301325
289.610351	13348.201197	28.306343
289.761732	13374.245776	28.311360
290.306661	13390.009845	28.316378
290.407353	13410.465044	28.321396
290.528950	13441.721658	28.326413
291.177465	13466.281484	28.331431
291.258282	13490.027552	28.336448
291.784384	13500.951874	28.341466
291.858858	13527.122897	28.346484
292.081815	13546.276758	28.351501
292.988661	13567.449748	28.356519
292.891500	13599.790902	28.361536
293.219833	13606.347879	28.366554
293.603946	13637.610271	28.371572
293.827960	13657.243188	28.376589
294.358514	13663.829756	28.381607
294.200326	13691.390178	28.386624
294.620910	13703.165803	28.391642
294.939457	13733.977465	28.396660
295.183435	13752.105265	28.401677
295.665186	13768.931352	28.406695
295.667254	13799.902690	28.411712
296.323987	13811.563658	28.416730
296.526719	13839.975522	28.421748
296.932055	13859.852895	28.426765
296.629527	13871.217217	28.431783
296.585566	13898.157042	28.436800
297.723700	13927.895683	28.441818
297.853954	13953.229170	28.446836
298.146472	13973.987439	28.451853
298.807024	13989.937835	28.456871
298.670059	14015.994915	28.461888
299.221638	14030.830226	28.466906
299.556350	14059.838428	28.471924
299.525544	14082.175948	28.476941
299.881488	14102.329717	28.481959
300.324494	14120.075103	28.486976
300.726486	14127.628762	28.491994
300.699432	14144.121804	28.497012
301.033129	14156.788416	28.502029
301.563800	14172.814075	28.507047
301.314945	14202.325740	28.512064
301.853734	14219.308335	28.517082
302.328930	14235.875941	28.522100
302.310880	14262.837293	28.527117
302.937722	14286.295556	28.532135
303.074179	14311.819273	28.537152
303.433524	14338.808120	28.542170
303.623993	14366.970758	28.547188
303.532980	14385.676383	28.552205
304.392834	14407.405139	28.557223
304.580688	14443.683493	28.562240
304.847531	14463.121161	28.567258
305.075500	14492.114699	28.572276
305.442864	14521.173476	28.577293
305.988037	14535.209661	28.582311
306.329894	14565.870880	28.587328
306.664769	14584.115372	28.592346
307.139941	14599.783410	28.597364
307.496859	14632.858395	28.602381
307.677122	14642.478991	28.607399
307.925173	14664.047723	28.612416
307.997989	14682.204884	28.617434
308.147529	14708.513522	28.622452
308.768773	14735.696086	28.627469
309.186044	14760.214179	28.632487
309.672072	14775.414064	28.637504
309.503889	14798.296985	28.642522
310.022398	14826.563725	28.647540
310.521255	14848.838260	28.652557
310.752681	14865.101686	28.657575
311.055426	14893.078000	28.662592
311.323036	14914.084304	28.667610
311.516801	14925.450740	28.672628
311.858102	14952.661087	28.677645
312.383737	14972.059676	28.682663
312.518020	14997.535959	28.687680
312.818200	15020.620639	28.692698
313.189173	15030.025491	28.697716
313.449249	15066.603764	28.702733
313.780805	15081.437045	28.707751
314.301121	15110.022353	28.712768
314.267274	15139.520600	28.717786
314.796347	15153.881513	28.722804
315.193760	15185.674240	28.727821
315.533061	15199.157172	28.732839
315.606518	15224.175761	28.737856
315.840497	15240.733874	28.742874
316.357827	15262.994882	28.747892
316.630525	15289.241508	28.752909
317.209766	15308.888535	28.757927
317.225987	15334.550377	28.762944
317.739098	15356.503284	28.767962
318.454311	15361.619376	28.772980
318.460145	15399.346930	28.777997
318.718809	15411.729040	28.783015
318.972964	15436.052903	28.788032
319.328374	15449.575931	28.793050
319.806554	15472.879243	28.798068
319.948454	15499.603365	28.803085
320.080228	15511.644034	28.808103
320.545193	15544.594216	28.813120
320.850838	15564.531140	28.818138
321.274323	15577.125673	28.823156
321.509647	15607.152356	28.828173
322.163655	15605.053458	28.833191
321.840069	15633.881808	28.838208
322.206195	15652.418637	28.843226
322.710768	15673.276358	28.848244
322.767946	15694.378385	28.853261
323.578856	15709.128165	28.858279
323.685351	15733.763774	28.863296
323.639737	15751.703712	28.868314
324.317820	15769.996745	28.873332
324.064552	15808.223639	28.878349
324.660922	15823.199751	28.883367
324.681769	15854.471328	28.888384
325.346722	15887.395400	28.893402
325.664583	15903.689681	28.898420
325.895047	15933.583785	28.903437
326.344965	15964.601713	28.908455
326.661482	15989.485084	28.913472
326.839785	16010.890590	28.918490
327.363444	16042.460745	28.923508
327.317025	16072.638938	28.928525
328.089143	16103.238115	28.933543
328.557641	16124.482250	28.938560
328.846704	16152.158757	28.943578
329.377026	16180.191012	28.948596
329.324390	16199.825473	28.953613
330.024746	16225.293501	28.958631
330.485319	16253.602234	28.963648
330.362830	16285.002381	28.968666
330.926171	16299.427981	28.973684
331.071774	16319.119618	28.978701
331.477313	16347.767057	28.983719
331.688835	16368.362066	28.988736
331.912789	16401.583984	28.993754
332.540311	16427.061227	28.998772
332.705137	16460.433336	29.003789
333.142314	16476.287573	29.008807
333.686459	16501.446140	29.013824
333.613985	16536.601027	29.018842
334.160610	16558.163805	29.023860
334.303373	16591.426339	29.028877
334.846494	16613.191533	29.033895
335.095626	16643.410120	29.038912
335.147150	16666.538262	29.043930
335.913812	16693.162486	29.048948
335.840896	16719.722372	29.053965
336.151671	16759.722849	29.058983
336.612172	16786.092096	29.064000
337.309858	16808.787197	29.069018
337.752674	16849.976630	29.074036
337.928969	16869.813590	29.079053
338.102066	16889.384708	29.084071
338.492456	16912.742418	29.089088
338.601703	16941.529774	29.094106
339.358129	16971.389144	29.099124
339.289267	17002.028296	29.104141
340.001244	17018.580015	29.109159
340.238136	17051.704940	29.114176
340.722744	17080.058400	29.119194
340.944754	17097.878261	29.124212
341.376356	17121.256242	29.129229
342.036994	17155.231812	29.134247
342.406381	17164.426923	29.139264
342.434081	17193.307030	29.144282
343.063432	17211.444218	29.149300
343.418266	17234.865015	29.154317
343.522111	17253.793848	29.159335
343.782535	17268.522647	29.164352
344.018870	17297.548106	29.169370
344.660892	17309.273912	29.174388
344.701942	17331.506201	29.179405
344.871325	17351.125769	29.184423
345.488008	17370.261478	29.189440
345.443243	17402.081216	29.194458
346.271400	17416.588498	29.199476
346.353897	17438.315943	29.204493
346.627403	17473.163332	29.209511
346.895058	17493.714194	29.214528
347.272524	17524.546842	29.219546
347.811350	17548.892905	29.224564
347.882611	17579.659685	29.229581
348.115396	17605.768417	29.234599
348.431306	17627.325062	29.239616
348.402903	17665.340883	29.244634
348.978888	17690.095590	29.249652
349.221362	17737.305885	29.254669
349.391232	17766.418830	29.259687
349.987563	17797.728086	29.264704
350.225935	17841.572195	29.269722
350.850193	17864.596178	29.274740
351.674541	17900.251837	29.279757
351.702395	17940.404449	29.284775
352.389849	17964.803768	29.289792
352.302093	17993.713830	29.294810
353.149253	18030.436372	29.299828
353.545051	18056.039603	29.304845
353.722447	18079.186712	29.309863
354.336651	18112.033757	29.314880
354.435822	18135.660510	29.319898
355.186354	18163.702243	29.324916
355.224669	18184.812135	29.329933
355.653854	18219.099337	29.334951
356.140228	18236.063229	29.339968
356.353878	18261.791509	29.344986
357.184549	18283.914875	29.350004
357.145799	18310.931963	29.355021
357.451439	18332.421859	29.360039
357.658392	18359.034203	29.365056
357.954130	18390.577193	29.370074
358.246998	18418.802300	29.375092
359.037586	18459.819933	29.380109
358.981796	18483.742399	29.385127
359.797082	18509.229606	29.390144
359.842119	18545.715576	29.395162
360.188624	18562.643046	29.400180
360.301478	18594.777910	29.405197
360.679646	18626.832665	29.410215
361.267515	18655.852758	29.415232
361.373163	18682.611654	29.420250
362.087720	18713.292973	29.425268
362.264479	18750.520603	29.430285
362.597661	18779.337133	29.435303
363.099186	18818.904260	29.440320
363.503566	18849.113772	29.445338
363.765055	18871.064121	29.450356
364.169478	18895.459626	29.455373
364.259672	18927.587844	29.460391
364.768984	18966.865534	29.465408
364.905432	19001.596917	29.470426
365.460784	19020.801436	29.475444
365.853187	19063.256435	29.480461
366.177017	19086.926176	29.485479
367.087529	19115.633547	29.490496
367.010285	19138.991379	29.495514
367.690008	19164.820483	29.500532
367.949197	19193.301563	29.505549
368.364356	19221.734807	29.510567
368.370318	19233.083258	29.515584
368.720751	19262.460585	29.520602
369.213707	19281.333625	29.525620
369.367925	19318.380218	29.530637
369.939675	19344.394582	29.535655
370.332922	19371.209455	29.540672
370.525315	19404.254982	29.545690
370.768461	19435.004613	29.550708
371.383967	19457.832030	29.555725
371.368376	19492.091406	29.560743
372.142010	19525.348400	29.565760
372.399564	19550.566902	29.570778
373.112346	19578.262542	29.575796
373.644205	19607.864273	29.580813
373.537366	19639.474670	29.585831
374.168978	19653.731089	29.590848
374.624363	19688.817865	29.595866
374.810913	19710.594107	29.600884
375.423916	19743.308980	29.605901
375.336907	19779.858906	29.610919
375.803091	19803.220741	29.615936
376.033743	19839.655160	29.620954
376.346545	19872.235509	29.625972
377.221233	19903.389137	29.630989
377.201707	19942.652587	29.636007
377.971906	19963.583683	29.641024
378.207143	20002.341590	29.646042
378.395099	20033.976463	29.651060
379.066370	20065.335908	29.656077
379.065029	20103.086339	29.661095
379.914663	20122.377433	29.666112
380.122043	20159.093879	29.671130
380.612306	20192.324997	29.676148
381.121119	20217.742564	29.681165
381.438681	20254.790992	29.686183
382.005090	20277.299717	29.691200
382.253301	20305.836532	29.696218
382.618450	20330.696272	29.701236
382.942584	20359.868606	29.706253
383.263564	20397.493829	29.711271
383.475812	20427.640235	29.716288
384.109396	20466.287563	29.721306
384.347997	20489.259174	29.726324
385.101921	20519.243573	29.731341
385.019673	20562.793126	29.736359
385.374514	20585.868609	29.741376
385.935444	20615.741646	29.746394
385.955071	20655.914735	29.751412
386.736632	20691.168778	29.756429
386.884287	20726.365411	29.761447
387.568876	20754.855993	29.766464
387.734487	20793.043878	29.771482
388.445886	20822.618040	29.776500
388.875574	20850.529762	29.781517
388.861811	20879.144015	29.786535
389.563740	20897.352046	29.791552
389.980276	20936.726961	29.796570
390.163159	20960.733279	29.801588
390.566248	20992.525127	29.806605
390.839794	21032.384323	29.811623
391.393403	21060.438283	29.816640
391.584693	21096.153504	29.821658
391.875069	21125.695392	29.826676
392.556762	21157.487167	29.831693
392.618969	21203.926634	29.836711
393.224776	21227.677287	29.841728
393.569687	21255.919053	29.846746
394.000861	21284.635372	29.851764
394.228972	21318.091844	29.856781
394.810988	21348.019452	29.861799
395.124300	21365.346275	29.866816
395.566430	21401.276056	29.871834
395.965070	21426.888700	29.876852
396.574191	21453.146120	29.881869
396.657351	21489.572252	29.886887
397.036155	21511.689538	29.891904
397.105999	21553.592435	29.896922
397.524630	21591.421750	29.901940
398.318242	21621.444118	29.906957
398.384439	21659.927922	29.911975
398.716263	21704.340592	29.916992
399.292723	21736.480416	29.922010
399.430006	21781.501000	29.927028
399.906959	21812.780759	29.932045
399.708356	21855.741111	29.937063
400.743946	21897.669514	29.942080
401.263837	21942.351270	29.947098
401.553512	21983.526645	29.952116
402.436369	22011.619151	29.957133
402.670528	22045.996902	29.962151
403.293975	22086.699442	29.967168
403.422384	22114.972166	29.972186
403.730887	22156.548504	29.977204
404.622447	22190.007277	29.982221
404.667892	22230.056839	29.987239
405.604784	22252.202571	29.992256
405.896140	22292.602631	29.997274
406.063246	22323.605059	30.002292
406.490732	22353.646747	30.007309
406.843143	22391.022071	30.012327
407.212500	22424.933553	30.017344
407.831221	22455.725876	30.022362
408.035322	22495.711964	30.027380
408.907313	22523.543791	30.032397
409.190655	22570.663131	30.037415
409.375920	22592.853281	30.042432
410.051733	22617.529369	30.047450
410.429854	22666.935473	30.052468
410.916282	22683.750907	30.057485
411.256238	22716.843148	30.062503
411.576406	22746.521696	30.067520
411.923227	22780.719875	30.072538
412.359797	22819.714257	30.077556
412.838710	22846.485792	30.082573
413.235629	22883.719224	30.087591
413.484558	22923.869201	30.092608
414.099867	22948.681934	30.097626
414.414019	22990.201033	30.102644
414.759339	23023.807045	30.107661
415.259158	23066.054080	30.112679
415.197808	23100.615326	30.117696
415.858414	23128.235560	30.122714
416.132570	23178.587564	30.127732
416.739798	23204.474293	30.132749
417.188648	23241.340382	30.137767
417.398256	23272.523580	30.142784
417.968346	23309.305100	30.147802
418.352052	23342.929042	30.152820
418.897931	23386.995307	30.157837
418.774811	23419.107443	30.162855
419.870101	23461.055068	30.167872
420.078707	23491.524490	30.172890
420.475896	23525.501368	30.177908
421.219545	23557.569668	30.182925
421.732370	23598.678910	30.187943
421.971647	23622.152967	30.192960
422.790392	23643.522148	30.197978
422.676183	23669.961057	30.202996
423.207232	23703.919292	30.208013
423.563283	23732.642727	30.213031
423.922479	23763.472487	30.218048
424.389996	23790.465012	30.223066
424.514353	23826.184434	30.228084
424.982693	23844.901082	30.233101
425.332250	23893.536457	30.238119
425.551155	23938.137651	30.243136
425.846772	23971.340593	30.248154
426.199029	24023.079352	30.253172
426.629281	24066.273943	30.258189
427.144753	24107.395010	30.263207
427.727429	24151.687398	30.268224
428.225170	24191.392321	30.273242
428.087995	24244.632030	30.278260
428.897160	24281.683595	30.283277
429.279986	24325.151622	30.288295
429.810071	24371.153283	30.293312
430.622454	24403.820524	30.298330
431.038075	24447.627222	30.303348
431.477130	24482.617822	30.308365
431.869137	24525.608582	30.313383
432.040633	24566.465966	30.318400
432.949470	24601.634543	30.323418
433.154966	24644.514535	30.328436
433.830151	24681.002486	30.333453
434.099529	24723.780636	30.338471
434.192242	24772.779573	30.343488
435.162737	24799.567447	30.348506
435.436968	24855.292615	30.353524
436.176868	24883.878764	30.358541
436.891624	24922.117510	30.363559
436.805200	24954.549744	30.368576
437.309654	24991.959223	30.373594
437.535779	25027.885096	30.378612
438.056294	25067.014230	30.383629
438.408857	25110.981302	30.388647
438.754006	25150.202729	30.393664
439.421000	25187.469033	30.398682
439.760868	25232.618169	30.403700
440.451656	25274.753898	30.408717
440.755134	25323.419879	30.413735
440.943150	25353.006542	30.418752
441.326050	25398.486489	30.423770
442.030999	25439.793882	30.428788
442.719544	25471.439617	30.433805
442.893393	25517.541154	30.438823
443.526975	25549.041571	30.443840
444.183503	25590.530822	30.448858
444.348854	25624.417754	30.453876
444.911917	25654.094272	30.458893
445.534696	25704.531639	30.463911
445.687453	25740.083169	30.468928
446.403602	25781.711264	30.473946
446.472132	25826.449492	30.478964
447.143940	25865.902378	30.483981
447.555200	25906.953531	30.488999
447.954773	25938.225272	30.494016
448.530644	25985.434928	30.499034
449.324814	26021.388734	30.504052
449.775115	26052.683832	30.509069
449.903590	26083.795670	30.514087
450.048562	26129.550340	30.519104
450.826499	26154.788733	30.524122
450.881936	26189.000932	30.529140
451.420590	26229.482917	30.534157
452.232635	26266.825343	30.539175
452.427857	26299.901145	30.544192
453.015304	26314.093215	30.549210
453.025357	26361.448003	30.554228
453.391633	26396.678503	30.559245
453.699619	26431.682144	30.564263
454.084513	26483.139011	30.569280
454.841433	26527.304597	30.574298
454.899513	26571.740507	30.579316
455.483711	26616.281887	30.584333
456.035083	26660.055982	30.589351
456.315356	26708.445812	30.594368
456.958298	26743.587074	30.599386
457.263887	26795.020140	30.604404
457.750965	26835.360667	30.609421
458.265410	26879.633523	30.614439
459.068535	26927.827038	30.619456
459.696864	26970.740632	30.624474
459.766939	27015.387045	30.629492
460.427877	27055.891739	30.634509
460.863332	27090.547552	30.639527
461.507946	27143.165265	30.644544
462.027447	27181.394025	30.649562
462.208783	27224.019447	30.654580
462.823453	27270.705698	30.659597
463.209299	27311.644520	30.664615
463.530216	27345.786680	30.669632
464.386509	27387.632049	30.674650
464.776618	27433.466316	30.679668
465.472688	27459.934673	30.684685
466.283206	27500.179063	30.689703
466.393701	27548.006272	30.694720
466.776883	27587.561327	30.699738
467.371708	27613.191780	30.704756
467.671650	27655.950056	30.709773
468.544148	27701.086903	30.714791
468.669025	27743.912220	30.719808
469.349922	27777.408902	30.724826
469.306806	27811.019148	30.729844
469.963502	27867.441540	30.734861
470.490901	27903.497039	30.739879
470.786396	27947.726833	30.744896
471.510298	27979.380781	30.749914
471.863569	28031.664532	30.754932
472.136784	28080.084591	30.759949
472.893878	28119.162564	30.764967
473.071084	28171.583129	30.769984
473.696838	28205.856353	30.775002
473.912764	28269.627721	30.780020
474.590388	28309.877052	30.785037
475.371312	28355.548126	30.790055
475.165832	28401.136479	30.795072
475.961367	28438.101446	30.800090
476.388612	28499.330668	30.805108
476.989751	28540.545923	30.810125
477.079075	28582.899661	30.815143
477.513226	28636.386426	30.820160
477.972534	28674.139440	30.825178
478.880404	28727.955063	30.830196
479.637415	28767.687548	30.835213
479.990286	28823.485031	30.840231
480.269793	28865.110769	30.845248
480.722904	28908.749051	30.850266
481.468609	28959.390076	30.855284
482.057767	28998.806987	30.860301
482.408902	29029.426646	30.865319
482.649304	29074.838861	30.870336
483.471221	29109.775472	30.875354
483.634312	29157.705655	30.880372
484.134905	29193.361281	30.885389
484.701980	29223.566963	30.890407
485.157053	29263.612396	30.895424
485.396930	29313.344360	30.900442
485.966524	29342.937781	30.905460
486.266863	29397.139941	30.910477
486.917137	29440.380954	30.915495
486.766083	29487.736194	30.920512
487.837467	29533.520035	30.925530
488.195537	29583.387800	30.930548
488.694357	29638.378148	30.935565
489.289886	29669.460124	30.940583
489.423053	29727.890223	30.945600
490.339894	29776.845783	30.950618
490.649077	29817.342546	30.955636
491.519761	29873.095548	30.960653
491.725199	29912.833569	30.965671
492.076306	29966.710432	30.970688
492.738593	30006.335208	30.975706
493.455107	30065.001177	30.980724
493.623053	30116.305905	30.985741
494.498991	30165.401831	30.990759
494.573918	30209.604431	30.995776
495.057653	30263.980843	31.000794
495.653016	30317.253606	31.005812
495.955826	30363.586422	31.010829
496.753872	30413.532028	31.015847
497.239066	30462.990022	31.020864
497.947643	30507.814193	31.025882
498.515114	30552.523002	31.030900
498.939063	30607.812735	31.035917
499.685962	30652.460556	31.040935
499.845857	30699.666638	31.045952
500.620978	30756.078752	31.050970
500.989421	30800.827435	31.055988
501.517026	30846.322913	31.061005
502.064693	30880.607990	31.066023
502.324511	30943.176536	31.071040
503.158930	30990.981700	31.076058
503.828422	31039.426396	31.081076
504.409308	31091.501763	31.086093
504.877327	31118.256362	31.091111
505.306697	31169.034993	31.096128
505.691667	31207.787038	31.101146
506.161613	31258.167961	31.106164
506.643591	31308.547037	31.111181
507.034253	31351.630622	31.116199
507.199714	31408.325554	31.121216
507.838002	31455.788955	31.126234
508.471783	31507.847333	31.131252
508.904285	31570.525203	31.136269
509.606635	31606.316418	31.141287
510.077564	31661.781531	31.146304
510.254482	31707.996719	31.151322
510.924271	31756.837750	31.156340
511.239555	31814.695598	31.161357
512.201475	31862.216977	31.166375
512.182361	31921.329540	31.171392
512.734270	31971.629515	31.176410
513.547105	32021.201740	31.181428
513.584760	32085.918882	31.186445
514.320454	32134.857334	31.191463
514.667462	32186.233106	31.196480
515.196505	32248.805894	31.201498
515.973187	32297.053285	31.206516
516.317394	32342.605049	31.211533
517.045260	32384.395262	31.216551
517.719671	32434.272383	31.221568
518.220087	32483.632539	31.226586
518.472013	32520.948494	31.231604
518.689276	32577.524994	31.236621
519.423316	32619.892194	31.241639
519.805086	32677.776564	31.246656
520.440047	32730.519927	31.251674
521.026068	32783.546074	31.256692
521.113494	32844.811918	31.261709
522.163153	32889.645649	31.266727
523.001319	32936.250038	31.271744
523.563260	32987.718784	31.276762
523.625699	33027.683109	31.281780
524.440709	33082.360482	31.286797
524.878968	33139.744739	31.291815
525.255987	33186.621735	31.296832
525.970009	33240.016200	31.301850
526.327272	33286.767348	31.306868
526.361422	33337.936298	31.311885
527.396685	33398.078435	31.316903
527.661131	33457.862351	31.321920
528.546341	33525.817860	31.326938
529.374476	33561.447050	31.331956
529.690682	33627.723620	31.336973
530.370798	33667.599796	31.341991
530.909342	33725.616257	31.347008
531.331006	33776.349972	31.352026
531.958347	33825.519284	31.357044
532.203781	33888.536069	31.362061
532.773627	33938.153848	31.367079
533.248689	33994.180958	31.372096
533.620585	34057.486675	31.377114
534.656698	34097.222857	31.382132
535.055889	34161.234468	31.387149
535.518061	34214.736638	31.392167
535.997823	34255.660281	31.397184
536.364833	34320.943254	31.402202
536.835449	34379.086683	31.407220
537.226777	34433.592149	31.412237
537.972919	34495.174377	31.417255
538.596708	34558.882002	31.422272
538.825671	34626.243373	31.427290
539.778095	34681.051231	31.432308
539.879733	34749.911073	31.437325
540.627794	34814.362761	31.442343
541.356491	34872.016950	31.447360
541.552446	34936.465753	31.452378
542.165336	34990.481801	31.457396
542.682386	35053.621843	31.462413
543.165445	35120.128796	31.467431
544.058378	35182.594847	31.472448
544.443207	35244.577116	31.477466
545.323252	35298.275318	31.482484
545.725218	35372.039550	31.487501
546.297537	35422.143890	31.492519
546.967990	35474.371894	31.497536
547.474677	35527.649691	31.502554
548.472463	35580.016358	31.507572
548.988198	35635.745197	31.512589
549.370636	35684.417292	31.517607
549.858924	35743.515332	31.522624
549.966501	35802.591343	31.527642
550.943042	35862.861939	31.532660
551.476500	35906.144346	31.537677
551.976541	35963.117128	31.542695
552.591361	36017.950208	31.547712
553.465795	36073.021393	31.552730
553.710464	36104.150597	31.557748
554.042369	36160.315454	31.562765
554.643095	36213.166267	31.567783
555.365335	36250.636255	31.572800
555.938416	36313.073936	31.577818
556.312337	36366.360396	31.582836
556.890455	36413.335635	31.587853
557.556030	36466.305861	31.592871
557.750142	36509.431243	31.597888
557.953124	36567.427182	31.602906
558.697222	36625.699892	31.607924
559.161415	36689.523520	31.612941
559.533744	36747.795012	31.617959
560.189501	36808.620523	31.622976
560.543157	36872.797645	31.627994
561.241552	36940.519231	31.633012
561.757130	37003.429619	31.638029
562.676177	37065.036212	31.643047
562.969748	37137.089632	31.648064
563.398107	37202.287662	31.653082
564.304105	37263.685617	31.658100
565.048475	37342.706978	31.663117
564.970758	37402.813103	31.668135
565.808339	37462.165125	31.673152
566.357004	37533.827557	31.678170
567.090431	37597.294195	31.683188
567.572548	37671.906753	31.688205
568.228248	37744.227769	31.693223
569.385422	37801.454275	31.698240
569.563348	37864.969569	31.703258
570.175350	37925.458857	31.708276
570.931177	37991.003242	31.713293
571.460941	38055.502607	31.718311
572.039419	38110.174425	31.723328
572.749867	38170.430443	31.728346
573.493497	38226.322086	31.733364
573.465957	38291.334304	31.738381
574.256833	38346.505133	31.743399
575.569210	38411.930541	31.748416
575.711342	38471.789171	31.753434
576.511170	38535.806797	31.758452
576.560182	38590.561343	31.763469
577.016517	38654.857175	31.768487
578.123943	38716.697032	31.773504
578.372129	38778.707672	31.778522
579.392830	38842.077454	31.783540
579.867505	38895.875489	31.788557
580.313534	38951.970109	31.793575
581.256456	39010.198625	31.798592
581.465419	39076.140421	31.803610
582.209608	39131.567564	31.808628
583.087192	39196.834134	31.813645
583.594085	39247.262897	31.818663
584.367193	39296.479791	31.823680
584.745665	39358.975904	31.828698
585.528601	39405.947078	31.833716
586.103299	39472.186491	31.838733
586.728473	39522.735337	31.843751
587.150449	39568.753352	31.848768
587.762267	39628.828467	31.853786
587.945568	39680.877690	31.858804
588.515824	39743.463336	31.863821
588.678108	39801.444718	31.868839
589.339740	39868.435108	31.873856
590.031960	39930.035244	31.878874
590.892716	39992.551578	31.883892
591.205439	40059.351005	31.888909
591.459909	40123.713797	31.893927
592.319196	40173.910021	31.898944
592.562673	40240.693152	31.903962
593.386949	40291.315346	31.908980
594.037166	40362.675314	31.913997
594.445479	40428.465861	31.919015
595.076259	40484.970241	31.924032
595.282256	40565.676182	31.929050
595.944260	40624.947559	31.934068
596.933896	40693.487222	31.939085
597.580448	40748.506062	31.944103
597.998005	40803.026277	31.949120
598.600759	40867.621320	31.954138
599.240086	40936.636559	31.959156
599.817749	41005.340250	31.964173
600.127031	41071.465167	31.969191
601.048839	41142.988420	31.974208
601.761938	41211.269534	31.979226
602.447471	41284.205711	31.984244
602.962715	41343.516304	31.989261
603.629588	41420.737005	31.994279
604.345007	41489.040859	31.999296
604.588960	41555.295122	32.004314
605.238264	41625.229978	32.009332
606.056417	41697.230296	32.014349
606.365177	41767.045234	32.019367
607.637234	41827.892787	32.024384
608.055004	41895.410756	32.029402
608.668044	41960.320463	32.034420
609.246157	42027.916570	32.039437
609.883357	42090.464367	32.044455
610.599765	42152.992955	32.049472
611.127049	42224.020527	32.054490
611.994099	42297.975679	32.059508
612.511971	42364.872617	32.064525
613.072351	42434.241155	32.069543
613.743239	42494.887269	32.074560
613.812838	42567.115835	32.079578
614.646021	42629.689850	32.084596
615.533955	42696.510969	32.089613
616.057331	42769.486125	32.094631
617.103956	42836.508814	32.099648
617.428156	42904.086968	32.104666
617.931318	42976.340106	32.109684
618.734053	43043.482821	32.114701
619.134349	43120.565250	32.119719
619.934027	43171.230963	32.124736
620.573312	43253.086146	32.129754
621.211538	43314.949589	32.134772
621.859837	43376.435845	32.139789
622.336417	43449.948681	32.144807
622.982291	43510.794836	32.149824
623.757754	43578.019764	32.154842
624.256051	43650.156331	32.159860
625.114522	43710.661698	32.164877
625.345442	43782.318881	32.169895
626.165154	43849.237508	32.174912
626.659151	43923.582883	32.179930
627.112434	43991.456195	32.184948
628.203419	44062.100701	32.189965
628.402422	44126.442322	32.194983
629.267728	44202.388204	32.200000
629.843049	44266.333352	32.205018
630.526243	44341.245849	32.210036
631.355652	44397.034606	32.215053
631.773592	44476.238389	32.220071
632.380393	44533.943113	32.225088
632.933981	44601.555749	32.230106
633.683570	44664.055679	32.235124
634.614954	44718.811786	32.240141
634.837122	44784.872706	32.245159
635.750291	44833.635909	32.250176
636.117198	44902.013070	32.255194
636.605091	44972.375551	32.260212
637.284984	45038.254274	32.265229
637.702583	45100.239047	32.270247
638.449514	45163.442072	32.275264
639.348035	45236.510021	32.280282
639.883916	45304.585972	32.285300
640.418762	45358.231732	32.290317
641.011297	45433.122523	32.295335
641.743122	45497.955381	32.300352
642.410462	45577.927749	32.305370
642.815807	45639.938426	32.310388
643.509773	45713.979911	32.315405
644.083442	45793.472923	32.320423
644.937680	45873.838762	32.325440
645.426445	45937.001828	32.330458
646.109109	46013.143118	32.335476
647.122697	46080.599695	32.340493
647.258032	46163.359314	32.345511
647.929997	46229.960331	32.350528
648.782117	46307.647369	32.355546
648.894977	46384.137043	32.360564
649.874941	46457.439394	32.365581
650.275656	46549.219864	32.370599
651.546805	46619.019948	32.375616
652.301158	46699.083709	32.380634
652.763524	46769.956047	32.385652
653.864128	46842.459924	32.390669
654.098258	46927.091809	32.395687
654.769073	46994.039913	32.400704
655.488004	47072.266862	32.405722
656.015777	47151.754210	32.410740
657.082290	47208.093117	32.415757
657.784312	47283.629967	32.420775
658.240901	47351.919026	32.425792
658.930561	47434.191403	32.430810
659.489252	47506.222175	32.435828
660.210207	47578.374804	32.440845
660.605183	47662.250675	32.445863
661.670716	47727.803358	32.450880
662.248606	47806.287193	32.455898
662.923858	47888.172308	32.460916
663.497031	47958.607550	32.465933
664.120654	48038.385915	32.470951
664.601938	48100.496273	32.475968
665.264443	48183.948042	32.480986
665.827289	48269.883187	32.486004
666.911081	48342.872439	32.491021
667.146413	48439.641385	32.496039
667.985170	48504.927907	32.501056
668.623152	48588.906600	32.506074
669.107098	48662.211063	32.511092
670.383904	48739.193480	32.516109
670.680138	48818.277592	32.521127
671.288504	48897.692544	32.526144
672.292778	48976.148535	32.531162
672.727252	49052.245116	32.536180
673.631329	49137.044402	32.541197
673.848491	49215.587367	32.546215
674.606097	49290.570240	32.551232
675.683417	49376.339956	32.556250
676.181344	49458.264269	32.561268
676.665465	49526.218580	32.566285
677.402313	49604.023375	32.571303
677.913951	49684.389300	32.576320
678.688043	49754.270443	32.581338
679.317982	49825.536966	32.586356
680.000550	49900.774669	32.591373
680.539666	49978.894788	32.596391
681.288684	50056.535157	32.601408
682.052395	50132.246742	32.606426
682.331577	50205.192986	32.611444
683.028376	50280.338218	32.616461
683.617613	50361.281603	32.621479
684.491845	50446.101062	32.626496
685.144538	50537.028247	32.631514
685.840312	50612.945624	32.636532
686.832092	50695.428357	32.641549
687.224873	50786.905081	32.646567
687.750684	50868.416987	32.651584
688.549088	50946.675002	32.656602
688.909666	51037.810790	32.661620
689.977415	51122.386412	32.666637
690.632099	51214.655705	32.671655
690.943297	51303.785693	32.676672
691.770666	51389.084514	32.681690
692.451995	51479.891350	32.686708
693.225309	51573.791559	32.691725
693.860887	51667.980338	32.696743
694.467580	51759.356760	32.701760
695.504430	51846.789826	32.706778
695.737446	51947.787321	32.711796
697.009714	52035.820363	32.716813
697.108148	52124.155382	32.721831
697.951267	52228.060572	32.726848
699.014949	52326.098637	32.731866
699.396729	52415.885386	32.736884
700.277482	52516.734447	32.741901
700.907685	52612.230122	32.746919
701.921817	52699.733948	32.751936
702.529683	52788.423621	32.756954
703.045440	52886.852074	32.761972
704.128047	52971.477492	32.766989
704.809644	53071.888521	32.772007
705.349118	53165.771887	32.777024
706.154395	53260.970093	32.782042
706.836715	53357.098891	32.787060
707.749550	53447.023646	32.792077
708.242632	53547.499882	32.797095
709.109828	53640.794273	32.802112
709.912498	53721.242444	32.807130
710.481552	53818.200950	32.812148
711.355732	53904.614995	32.817165
711.859336	54002.615096	32.822183
712.484463	54099.312983	32.827200
713.040664	54188.706211	32.832218
713.712327	54286.623060	32.837236
714.804733	54373.483252	32.842253
715.203688	54471.572495	32.847271
715.764732	54565.010365	32.852288
716.824143	54666.826577	32.857306
717.439715	54777.233986	32.862324
718.430252	54868.314970	32.867341
718.912496	54958.052474	32.872359
720.016169	55059.117802	32.877376
721.024633	55143.234070	32.882394
721.427521	55228.506072	32.887412
722.401223	55321.759201	32.892429
722.883236	55403.543631	32.897447
723.636829	55503.708706	32.902464
724.455017	55584.616846	32.907482
724.847334	55677.595016	32.912500
725.725276	55749.628776	32.917517
726.534604	55839.815345	32.922535
726.940110	55918.903798	32.927552
727.846186	56006.124238	32.932570
728.234994	56091.945694	32.937588
728.970344	56182.809536	32.942605
729.644072	56269.380806	32.947623
730.308387	56365.735731	32.952640
731.500346	56451.956675	32.957658
732.076435	56547.189656	32.962676
732.528209	56633.691800	32.967693
733.397485	56727.727082	32.972711
733.879132	56823.248721	32.977728
734.501941	56918.317767	32.982746
735.430868	57024.780607	32.987764
736.098439	57120.885871	32.992781
736.805977	57214.078149	32.997799
737.244306	57317.451455	33.002816
738.579465	57404.537521	33.007834
738.590111	57525.076277	33.012852
739.694430	57620.094284	33.017869
740.569836	57719.315070	33.022887
741.494322	57826.320052	33.027904
742.269740	57912.293909	33.032922
742.846395	58027.389496	33.037940
743.762814	58126.782457	33.042957
744.457163	58224.803388	33.047975
745.040994	58334.003423	33.052992
745.997387	58422.167691	33.058010
746.652077	58522.970934	33.063028
747.560324	58621.331272	33.068045
748.451726	58725.047648	33.073063
748.963102	58833.567208	33.078080
749.812486	58926.181506	33.083098
750.553052	59035.081341	33.088116
751.055487	59132.980437	33.093133
752.026871	59234.038197	33.098151
752.538800	59339.337260	33.103168
753.804629	59438.154339	33.108186
754.243665	59550.785013	33.113204
754.964582	59645.294557	33.118221
756.059595	59753.792033	33.123239
756.823457	59844.737240	33.128256
757.603182	59950.405984	33.133274
758.367784	60063.781982	33.138292
759.007759	60153.175358	33.143309
760.319372	60249.960062	33.148327
760.476199	60359.127890	33.153344
761.619277	60456.029935	33.158362
762.246037	60559.382343	33.163380
763.068821	60656.382564	33.168397
763.777925	60757.004630	33.173415
764.615781	60857.283559	33.178432
765.325919	60944.500925	33.183450
766.211588	61050.657167	33.188468
766.994226	61151.667204	33.193485
767.506062	61244.057168	33.198503
768.268051	61357.946437	33.203520
769.072008	61452.134610	33.208538
770.255457	61557.789154	33.213556
771.112959	61659.743722	33.218573
771.660765	61746.820707	33.223591
772.400639	61845.565819	33.228608
773.225933	61952.779637	33.233626
773.995480	62041.009483	33.238644
774.371293	62143.829901	33.243661
775.490947	62247.393746	33.248679
776.057587	62346.637660	33.253696
776.835453	62436.378501	33.258714
777.599837	62525.091664	33.263732
777.922911	62626.798107	33.268749
778.859383	62718.233227	33.273767
779.397446	62812.749746	33.278784
780.308853	62903.576702	33.283802
780.994211	63016.760935	33.288820
781.464467	63126.903017	33.293837
782.677540	63216.967180	33.298855
782.908869	63324.128360	33.303872
783.707096	63426.316408	33.308890
784.642041	63543.021043	33.313908
785.329922	63646.808726	33.318925
786.569251	63750.790174	33.323943
787.162201	63866.453305	33.328960
788.036513	63972.715010	33.333978
788.909253	64096.102030	33.338996
789.428075	64195.002417	33.344013
790.782086	64278.871914	33.349031
791.014973	64411.083849	33.354048
791.915710	64525.713600	33.359066
792.714361	64635.980064	33.364084
793.270084	64752.507690	33.369101
794.329413	64853.344702	33.374119
795.198539	64975.536440	33.379136
796.190192	65078.825880	33.384154
797.151806	65181.830003	33.389172
797.721328	65303.264042	33.394189
798.741954	65407.207774	33.399207
799.352594	65513.603142	33.404224
800.403890	65624.591660	33.409242
800.808010	65737.331488	33.414260
801.692615	65853.747645	33.419277
802.943147	65951.207744	33.424295
803.379881	66080.216611	33.429312
804.608292	66180.779190	33.434330
805.281365	66300.096668	33.439348
805.901350	66411.754964	33.444365
807.165431	66516.770296	33.449383
807.584473	66626.793944	33.454400
807.943882	66746.279631	33.459418
809.196187	66844.173493	33.464436
809.927534	66971.659714	33.469453
811.052228	67070.707413	33.474471
811.737668	67195.199515	33.479488
812.343840	67298.835510	33.484506
813.453269	67415.912267	33.489524
814.271482	67534.359216	33.494541
814.910176	67634.710166	33.499559
815.692140	67758.272873	33.504576
816.671842	67857.126959	33.509594
817.801409	67972.894720	33.514612
818.391977	68092.842948	33.519629
819.164289	68204.947085	33.524647
819.911212	68319.161445	33.529664
820.706721	68432.976379	33.534682
821.560450	68540.605035	33.539700
822.415318	68657.408305	33.544717
823.343352	68758.519705	33.549735
824.116796	68883.525639	33.554752
824.826546	68996.270255	33.559770
825.906375	69107.070051	33.564788
826.645120	69218.508541	33.569805
827.498122	69327.930676	33.574823
828.286829	69440.417989	33.579840
828.990236	69549.025048	33.584858
829.720621	69660.498844	33.589876
830.276103	69777.610689	33.594893
831.741418	69878.575310	33.599911
832.489358	69991.666637	33.604928
832.959600	70093.119325	33.609946
834.169823	70189.878458	33.614964
834.623635	70293.004127	33.619981
835.614810	70398.690849	33.624999
835.965794	70514.715010	33.630016
837.094300	70617.408163	33.635034
838.069647	70739.571367	33.640052
838.593562	70840.797396	33.645069
839.757267	70952.832257	33.650087
840.031242	71075.005868	33.655104
840.953467	71192.292419	33.660122
841.869827	71306.216479	33.665140
842.441566	71424.883873	33.670157
843.727219	71542.371487	33.675175
844.047379	71664.597709	33.680192
844.906410	71793.394287	33.685210
846.168696	71908.826254	33.690228
846.503917	72034.998048	33.695245
847.652425	72155.249842	33.700263
848.479735	72291.605183	33.705280
849.227689	72418.583630	33.710298
850.248626	72540.047537	33.715316
850.999147	72674.527150	33.720333
852.060690	72788.321172	33.725351
852.820138	72926.272703	33.730368
853.904194	73048.114773	33.735386
854.891386	73176.531575	33.740404
855.729394	73293.856081	33.745421
856.461884	73418.844518	33.750439
857.666047	73546.057653	33.755456
858.215612	73671.659612	33.760474
859.164648	73802.331494	33.765492
859.860933	73919.391886	33.770509
860.665765	74048.248728	33.775527
861.460088	74186.626184	33.780544
861.989090	74319.210999	33.785562
863.288247	74444.370877	33.790580
864.162549	74584.331366	33.795597
865.138329	74696.815059	33.800615
866.105925	74839.493920	33.805632
866.904204	74971.121080	33.810650
867.866003	75101.128186	33.815668
868.427055	75231.018922	33.820685
869.409306	75344.636967	33.825703
870.264161	75490.722389	33.830720
871.092682	75628.483440	33.835738
872.324717	75751.460845	33.840756
873.063640	75885.898835	33.845773
874.512296	76010.638108	33.850791
875.057617	76126.906654	33.855808
875.931183	76255.429826	33.860826
877.028729	76377.598065	33.865844
877.791941	76509.404639	33.870861
878.658491	76631.916082	33.875879
879.650881	76752.547819	33.880896
880.559135	76883.200437	33.885914
881.565937	77003.970308	33.890932
882.205852	77131.120358	33.895949
882.925647	77255.835368	33.900967
884.001965	77376.589438	33.905984
884.935574	77511.175850	33.911002
885.472711	77628.687031	33.916020
886.702908	77750.619487	33.921037
887.185777	77876.003354	33.926055
888.308350	78009.897354	33.931072
888.930388	78134.051495	33.936090
889.987021	78244.952128	33.941108
890.704373	78379.516274	33.946125
891.386123	78491.422628	33.951143
892.247944	78614.489731	33.956160
893.026753	78741.056658	33.961178
893.960668	78869.496346	33.966196
894.581526	78989.866341	33.971213
895.705609	79123.159468	33.976231
896.212650	79249.470563	33.981248
896.966109	79393.643654	33.986266
897.939635	79520.442118	33.991284
898.590059	79664.317684	33.996301
899.858058	79800.779263	34.001319
900.480574	79943.838853	34.006336
901.159199	80099.978577	34.011354
902.242548	80233.038277	34.016372
903.161185	80391.607476	34.021389
904.103084	80536.737230	34.026407
905.199766	80675.433904	34.031424
905.918070	80821.013651	34.036442
907.107450	80965.453617	34.041460
907.938787	81113.211750	34.046477
908.977914	81257.090069	34.051495
909.953888	81404.743930	34.056512
910.686160	81541.298238	34.061530
912.068239	81676.891833	34.066548
912.690354	81827.694253	34.071565
913.625378	81979.167145	34.076583
914.637639	82122.138008	34.081600
915.135446	82266.953636	34.086618
916.549657	82411.789450	34.091636
917.585214	82567.260699	34.096653
918.418705	82704.792167	34.101671
919.704420	82851.613293	34.106688
920.034557	83007.577453	34.111706
921.208248	83138.532311	34.116724
922.051416	83297.020251	34.121741
923.035256	83435.372695	34.126759
924.517973	83577.831923	34.131776
924.937410	83728.433569	34.136794
926.151035	83861.777538	34.141812
927.087023	84011.359200	34.146829
927.856246	84159.387623	34.151847
928.771833	84306.393095	34.156864
929.986734	84442.498841	34.161882
931.165926	84579.503431	34.166900
931.741055	84731.572744	34.171917
932.816234	84872.860853	34.176935
933.660392	85011.195182	34.181952
934.412777	85161.143630	34.186970
935.452834	85295.239528	34.191988
936.355144	85448.246490	34.197005
937.560428	85602.223083	34.202023
938.264451	85748.848698	34.207040
938.963892	85896.089766	34.212058
940.260189	86043.897462	34.217076
941.429712	86185.253840	34.222093
942.225752	86337.335034	34.227111
943.166969	86477.547642	34.232128
943.644014	86629.772066	34.237146
944.902690	86779.172562	34.242164
946.017821	86919.871602	34.247181
946.622585	87068.736625	34.252199
947.805288	87209.198414	34.257216
948.179011	87355.831717	34.262234
949.545339	87504.908937	34.267252
950.343481	87671.508570	34.272269
951.415739	87807.967525	34.277287
952.198064	87937.545888	34.282304
952.912729	88089.480967	34.287322
954.069089	88228.567290	34.292340
954.975372	88367.233818	34.297357
955.774532	88507.886970	34.302375
957.160696	88646.254281	34.307392
958.030458	88790.422311	34.312410
958.704483	88934.553967	34.317428
959.946080	89083.408591	34.322445
960.361091	89230.147885	34.327463
961.546101	89364.312539	34.332480
962.349373	89528.614411	34.337498
963.386339	89669.614800	34.342516
964.349083	89820.146573	34.347533
965.047032	89984.355069	34.352551
966.504396	90128.813722	34.357568
967.565089	90287.141877	34.362586
968.527478	90444.265871	34.367604
969.745240	90589.273217	34.372621
970.402034	90743.563741	34.377639
971.638187	90889.190082	34.382656
972.202100	91050.573667	34.387674
973.714838	91199.668724	34.392692
974.818713	91354.300607	34.397709
975.694041	91508.154818	34.402727
976.606000	91645.238092	34.407744
977.238271	91806.267309	34.412762
978.253690	91963.556968	34.417780
979.268703	92120.429982	34.422797
980.270428	92283.015224	34.427815
980.937354	92434.295764	34.432832
982.236065	92616.360112	34.437850
983.105991	92768.444636	34.442868
984.126715	92936.119943	34.447885
985.008721	93096.458127	34.452903
986.392160	93247.137852	34.457920
987.301846	93410.859823	34.462938
988.327966	93572.487518	34.467956
989.368718	93731.360454	34.472973
990.255902	93886.468318	34.477991
991.515489	94043.984182	34.483008
992.267851	94213.915351	34.488026
993.260989	94371.205186	34.493044
994.435130	94538.669847	34.498061
995.191171	94699.121604	34.503079
996.253032	94849.820018	34.508096
997.280511	95023.357319	34.513114
998.339374	95184.395152	34.518132
999.350763	95340.555061	34.523149
1000.140269	95515.053015	34.528167
1001.446473	95671.267539	34.533184
1002.338739	95833.141058	34.538202
1003.701158	95997.147145	34.543220
1004.661503	96157.973360	34.548237
1005.562022	96329.584720	34.553255
1006.823337	96476.740363	34.558272
1007.537236	96642.845664	34.563290
1008.847487	96795.831730	34.568308
1009.782909	96955.097247	34.573325
1010.682115	97119.123990	34.578343
1012.092223	97278.351055	34.583360
1012.960972	97437.143203	34.588378
1013.555556	97592.012370	34.593396
1015.063922	97739.698009	34.598413
1015.842544	97899.945044	34.603431
1017.111910	98053.319047	34.608448
1017.996523	98211.537355	34.613466
1018.958481	98368.857547	34.618484
1020.072266	98514.283217	34.623501
1021.041820	98652.978486	34.628519
1022.378545	98791.373229	34.633536
1023.072002	98938.928394	34.638554
1023.704084	99084.285039	34.643572
1025.049080	99227.346756	34.648589
1025.759724	99382.403957	34.653607
1026.687994	99530.214960	34.658624
1027.871200	99682.903986	34.663642
1028.748121	99841.969446	34.668660
1030.266231	100001.987199	34.673677
1030.557239	100154.889881	34.678695
1031.752116	100306.624685	34.683712
1032.506466	100475.394947	34.688730
1033.272205	100640.789797	34.693748
1034.677287	100800.014478	34.698765
1035.511169	100971.256778	34.703783
1036.886826	101135.395306	34.708800
1037.655665	101304.630822	34.713818
1038.536617	101475.083576	34.718836
1039.804501	101638.533991	34.723853
1040.295097	101817.753238	34.728871
1041.594740	101994.706163	34.733888
1042.765396	102179.425394	34.738906
1043.851299	102352.287782	34.743924
1045.009595	102522.714246	34.748941
1045.748400	102705.761033	34.753959
1047.293725	102874.454190	34.758976
1047.758834	103056.237980	34.763994
1049.166378	103236.163897	34.769012
1050.160281	103410.688528	34.774029
1050.988780	103598.969720	34.779047
1052.181329	103784.000662	34.784064
1053.315645	103971.208157	34.789082
1054.468671	104155.830334	34.794100
1055.586950	104333.114079	34.799117
1056.253507	104518.705760	34.804135
1057.613188	104707.261694	34.809152
1058.657525	104890.488542	34.814170
1059.744548	105069.454178	34.819188
1061.081403	105250.608769	34.824205
1061.943760	105442.798400	34.829223
1062.838038	105628.423556	34.834240
1064.414399	105812.290750	34.839258
1065.262601	105988.173749	34.844276
1066.700014	106170.584546	34.849293
1067.793875	106353.319373	34.854311
1068.919671	106529.717343	34.859328
1069.813580	106703.773659	34.864346
1070.711587	106891.205547	34.869364
1072.254937	107067.854684	34.874381
1072.960239	107254.953669	34.879399
1074.376305	107427.142458	34.884416
1075.601084	107609.357585	34.889434
1076.680003	107786.594893	34.894452
1077.967563	107946.800657	34.899469
1078.881206	108128.108100	34.904487
1080.116705	108301.839651	34.909504
1081.259705	108480.071582	34.914522
1081.836879	108649.252909	34.919540
1083.673015	108829.411880	34.924557
1084.460376	108989.503865	34.929575
1085.492103	109164.934004	34.934592
1086.745404	109331.993773	34.939610
1087.702483	109508.147823	34.944628
1088.830589	109678.067839	34.949645
1089.903152	109858.182542	34.954663
1091.147941	110016.292196	34.959680
1092.100771	110184.407589	34.964698
1092.859472	110340.256020	34.969716
1094.097669	110488.653570	34.974733
1095.170688	110661.236323	34.979751
1096.122914	110829.102423	34.984768
1097.276578	110994.896740	34.989786
1097.692735	111154.201384	34.994804
1098.895752	111327.881603	34.999821
1099.952945	111507.084929	35.004839
1101.376553	111689.015816	35.009856
1102.249246	111858.776217	35.014874
1103.229042	112048.168372	35.019892
1103.924994	112215.895263	35.024909
1104.979344	112403.795331	35.029927
1106.297458	112582.911817	35.034944
1107.667338	112769.951417	35.039962
1108.202798	112968.405320	35.044980
1109.369317	113154.987050	35.049997
1110.614621	113353.567045	35.055015
1111.519845	113542.170898	35.060032
1113.091953	113734.301773	35.065050
1114.186396	113935.622008	35.070068
1115.299064	114132.772516	35.075085
1116.274348	114315.656193	35.080103
1117.113648	114512.879898	35.085120
1118.570121	114710.585747	35.090138
1119.662644	114910.304257	35.095156
1120.817978	115093.429275	35.100173
1122.173244	115305.865443	35.105191
1123.219023	115500.857384	35.110208
1124.246985	115699.743263	35.115226
1125.629537	115896.405350	35.120244
1126.582436	116094.052072	35.125261
1127.646084	116291.149710	35.130279
1128.758391	116497.109828	35.135296
1130.116643	116704.411836	35.140314
1131.314529	116906.813068	35.145332
1132.429703	117098.763570	35.150349
1133.289502	117297.979808	35.155367
1134.501060	117515.980573	35.160384
1135.894482	117716.784026	35.165402
1136.833458	117933.946065	35.170420
1138.303657	118124.793040	35.175437
1138.934220	118334.077060	35.180455
1140.340838	118531.323435	35.185472
1141.687314	118743.469776	35.190490
1142.660181	118951.637282	35.195508
1143.910401	119152.271631	35.200525
1144.888417	119356.272292	35.205543
1146.641321	119566.266651	35.210560
1147.861681	119760.827769	35.215578
1148.623555	119968.505206	35.220596
1150.164386	120168.731019	35.225613
1151.044357	120366.203594	35.230631
1152.330365	120569.870346	35.235648
1153.197307	120774.342767	35.240666
1154.309480	120989.154590	35.245684
1155.731145	121175.302812	35.250701
1156.562548	121378.353327	35.255719
1157.583333	121583.502898	35.260736
1159.191171	121787.492350	35.265754
1160.175221	121999.608094	35.270772
1161.464107	122204.413495	35.275789
1162.356327	122409.361914	35.280807
1163.316501	122620.522896	35.285824
1164.658569	122827.871038	35.290842
1165.757058	123035.539691	35.295860
1167.285058	123228.666048	35.300877
1168.210066	123435.605762	35.305895
1169.084135	123625.978626	35.310912
1170.329779	123818.319012	35.315930
1171.574276	124025.336702	35.320948
1172.812630	124215.589704	35.325965
1174.037739	124418.139526	35.330983
1174.962452	124618.129574	35.336000
1175.895653	124816.586006	35.341018
1177.333588	125018.775141	35.346036
1178.548129	125217.327097	35.351053
1179.454980	125424.194699	35.356071
1180.348573	125639.037935	35.361088
1181.800376	125842.839864	35.366106
1182.567838	126058.796885	35.371124
1184.330432	126273.488251	35.376141
1185.391423	126490.996768	35.381159
1186.406932	126697.310003	35.386176
1187.910716	126906.015468	35.391194
1189.219254	127137.455125	35.396212
1190.008143	127340.438634	35.401229
1191.657028	127551.570721	35.406247
1192.583819	127776.525319	35.411264
1193.637164	127982.992977	35.416282
1194.759983	128215.713545	35.421300
1195.943060	128439.679931	35.426317
1197.242949	128656.074083	35.431335
1198.866063	128880.122993	35.436352
1200.099873	129104.427993	35.441370
1201.395147	129327.469547	35.446388
1202.572784	129541.215454	35.451405
1203.779929	129759.964890	35.456423
1204.818485	129978.046534	35.461440
1206.054759	130197.250518	35.466458
1207.483320	130421.317209	35.471476
1208.760557	130642.963994	35.476493
1210.030145	130865.779808	35.481511
1211.311480	131079.886580	35.486528
1212.792953	131300.540785	35.491546
1214.083627	131519.402633	35.496564
1215.659131	131731.158020	35.501581
1216.509262	131950.539320	35.506599
1217.606053	132157.851073	35.511616
1219.067121	132380.049981	35.516634
1220.077454	132590.877633	35.521652
1221.527440	132799.149291	35.526669
1223.316655	133023.669000	35.531687
1224.140381	133238.322185	35.536704
1225.464511	133444.628480	35.541722
1226.747750	133657.661853	35.546740
1227.253845	133870.761692	35.551757
1228.687690	134096.209628	35.556775
1229.994666	134312.108482	35.561792
1231.588221	134528.569921	35.566810
1232.383036	134749.602048	35.571828
1233.553147	134970.155258	35.576845
1234.774491	135185.452801	35.581863
1235.921303	135407.369335	35.586880
1237.461190	135629.273101	35.591898
1238.595067	135865.039376	35.596916
1239.802028	136085.327706	35.601933
1241.175423	136303.054310	35.606951
1242.436507	136519.913411	35.611968
1243.697500	136740.780364	35.616986
1244.617267	136961.565717	35.622004
1245.693612	137190.948182	35.627021
1247.270743	137405.085581	35.632039
1248.234353	137647.498268	35.637056
1249.378162	137867.301635	35.642074
1250.634531	138080.811694	35.647092
1251.640755	138286.161044	35.652109
1252.961496	138492.600786	35.657127
1254.545459	138728.147997	35.662144
1255.583060	138928.804716	35.667162
1256.662813	139151.061455	35.672180
1257.668283	139365.407207	35.677197
1258.757923	139593.269556	35.682215
1260.128457	139829.899399	35.687232
1261.097327	140046.487102	35.692250
1262.431998	140282.149652	35.697268
1263.974508	140516.245188	35.702285
1265.027865	140733.774255	35.707303
1266.102326	140985.524896	35.712320
1267.272644	141221.284432	35.717338
1268.651994	141455.603507	35.722356
1269.524084	141697.552846	35.727373
1270.835593	141941.599601	35.732391
1272.056411	142197.773011	35.737408
1273.648279	142441.738883	35.742426
1274.720260	142697.509411	35.747444
1276.390812	142944.876907	35.752461
1277.820663	143201.289399	35.757479
1278.995512	143445.914497	35.762496
1280.448606	143693.094930	35.767514
1281.619387	143941.427016	35.772532
1282.849255	144194.392431	35.777549
1284.422412	144440.137920	35.782567
1285.434781	144692.851153	35.787584
1286.589388	144947.115180	35.792602
1288.023498	145199.559383	35.797620
1289.285256	145452.731346	35.802637
1290.674135	145703.537941	35.807655
1292.076103	145965.783217	35.812672
1293.425910	146216.143285	35.817690
1294.799944	146481.148913	35.822708
1296.003314	146743.026816	35.827725
1297.625161	146995.871060	35.832743
1299.127623	147258.514903	35.837760
1300.346392	147495.829908	35.842778
1301.604883	147751.225198	35.847796
1302.875205	148006.950058	35.852813
1304.622769	148256.941322	35.857831
1305.656513	148514.611216	35.862848
1306.792420	148762.753846	35.867866
1308.462629	149017.785472	35.872884
1309.532954	149270.647726	35.877901
1311.018508	149519.206896	35.882919
1312.231030	149790.084625	35.887936
1313.701929	150026.866862	35.892954
1315.052905	150286.690807	35.897972
1316.209805	150538.494601	35.902989
1317.954025	150785.357882	35.908007
1319.161492	151040.644658	35.913024
1320.537991	151300.484056	35.918042
1322.251756	151549.336022	35.923060
1323.395611	151783.671935	35.928077
1325.026549	152030.435208	35.933095
1326.193147	152281.246936	35.938112
1327.895661	152524.627605	35.943130
1329.058143	152758.852258	35.948148
1330.455190	153009.998507	35.953165
1331.761876	153249.022353	35.958183
1332.781234	153490.949172	35.963200
1334.404511	153736.583061	35.968218
1335.383915	153974.511180	35.973236
1336.698694	154227.898736	35.978253
1338.251498	154460.001563	35.983271
1338.876011	154692.880744	35.988288
1340.571751	154925.051501	35.993306
1341.911416	155155.189451	35.998324
1342.748111	155394.989119	36.003341
1344.255911	155624.340917	36.008359
1345.249916	155878.020469	36.013376
1346.785914	156109.729878	36.018394
1348.135226	156357.442413	36.023412
1349.316075	156610.055557	36.028429
1350.338377	156845.025514	36.033447
1351.871134	157112.945894	36.038464
1353.234545	157363.237519	36.043482
1354.590298	157612.935736	36.048500
1355.446562	157869.213219	36.053517
1357.110328	158131.955575	36.058535
1358.451669	158393.661921	36.063552
1359.441472	158657.521260	36.068570
1360.902971	158920.961826	36.073588
1362.419165	159184.293561	36.078605
1363.689475	159454.924232	36.083623
1365.134735	159735.600823	36.088640
1366.173554	160009.254716	36.093658
1367.663109	160280.120993	36.098676
1368.870123	160560.931372	36.103693
1370.274959	160834.822024	36.108711
1371.537034	161117.517393	36.113728
1372.819794	161406.986099	36.118746
1374.465848	161675.729551	36.123764
1375.682793	161963.284539	36.128781
1377.138695	162251.372924	36.133799
1378.801744	162546.686183	36.138816
1379.960423	162825.806915	36.143834
1381.604642	163105.572427	36.148852
1383.031141	163402.212155	36.153869
1384.726541	163679.156326	36.158887
1386.010620	163969.784198	36.163904
1387.492122	164241.349677	36.168922
1388.891996	164519.058609	36.173940
1390.408420	164822.278285	36.178957
1391.889326	165105.826746	36.183975
1393.095083	165390.589833	36.188992
1395.167149	165671.874607	36.194010
1396.264269	165957.496758	36.199028
1397.327402	166244.509416	36.204045
1399.136762	166508.929329	36.209063
1400.529588	166789.090020	36.214080
1402.354154	167083.544671	36.219098
1403.836640	167356.004806	36.224116
1404.971556	167633.383848	36.229133
1406.760702	167907.268567	36.234151
1407.891405	168183.750799	36.239168
1409.450013	168464.161059	36.244186
1411.169433	168723.507950	36.249204
1412.189165	169016.522138	36.254221
1413.762998	169291.339070	36.259239
1415.280756	169567.334343	36.264256
1416.650088	169846.591609	36.269274
1418.181994	170123.907596	36.274292
1419.567001	170394.853986	36.279309
1420.692419	170670.095892	36.284327
1422.102573	170943.338164	36.289344
1423.295620	171227.937212	36.294362
1424.809584	171503.360950	36.299380
1426.214117	171794.869862	36.304397
1427.521460	172055.369546	36.309415
1429.284862	172355.172661	36.314432
1430.424965	172633.811946	36.319450
1431.913665	172903.448641	36.324468
1433.269917	173185.240695	36.329485
1434.531344	173435.768275	36.334503
1436.003930	173718.787909	36.339520
1437.116718	173989.127373	36.344538
1438.609669	174255.243016	36.349556
1439.757309	174525.313222	36.354573
1441.677379	174808.785626	36.359591
1442.778010	175084.146058	36.364608
1443.937587	175363.521315	36.369626
1445.516526	175647.613361	36.374644
1447.044531	175933.720651	36.379661
1448.203353	176224.827448	36.384679
1449.196836	176513.932689	36.389696
1450.540157	176809.378198	36.394714
1452.091172	177102.760526	36.399732
1453.429156	177420.889957	36.404749
1455.154770	177717.153365	36.409767
1456.517809	178019.519613	36.414784
1457.988437	178336.972946	36.419802
1459.697141	178635.097506	36.424820
1460.778750	178959.802519	36.429837
1462.244519	179259.798486	36.434855
1463.656068	179583.704109	36.439872
1465.239694	179903.648800	36.444890
1466.937466	180205.921884	36.449908
1468.107989	180523.907922	36.454925
1469.945671	180839.107590	36.459943
1471.368215	181159.340453	36.464960
1472.912923	181485.342819	36.469978
1474.656304	181790.790609	36.474996
1475.811948	182123.499361	36.480013
1477.177071	182441.794808	36.485031
1479.390651	182756.042595	36.490048
1480.273343	183082.506819	36.495066
1481.797149	183407.432787	36.500084
1483.012460	183735.166045	36.505101
1484.523967	184061.240319	36.510119
1486.374234	184393.200932	36.515136
1487.636052	184732.368962	36.520154
1489.336560	185059.293758	36.525172
1491.244538	185403.081023	36.530189
1492.507505	185733.217332	36.535207
1494.427913	186048.865247	36.540224
1495.512711	186376.889585	36.545242
1497.639553	186697.419430	36.550260
1498.728885	187029.470679	36.555277
1500.459261	187356.949736	36.560295
1501.961380	187670.505156	36.565312
1503.162928	187994.952547	36.570330
1505.213463	188319.578834	36.575348
1506.454785	188643.109319	36.580365
1507.776783	188976.123473	36.585383
1509.921117	189292.221922	36.590400
1511.003997	189622.638860	36.595418
1512.630803	189943.243912	36.600436
1514.188224	190278.828859	36.605453
1515.552439	190594.085681	36.610471
1517.175470	190919.203136	36.615488
1519.016966	191253.489841	36.620506
1520.601865	191566.734929	36.625524
1521.783810	191895.408845	36.630541
1523.287762	192217.112652	36.635559
1524.833893	192528.109394	36.640576
1525.926241	192862.465198	36.645594
1527.627793	193185.588625	36.650612
1528.974338	193522.267247	36.655629
1530.584566	193850.284108	36.660647
1532.521245	194167.470509	36.665664
1533.822701	194493.129636	36.670682
1535.456661	194795.490335	36.675700
1537.008207	195104.518467	36.680717
1538.193329	195408.301927	36.685735
1539.828205	195718.220613	36.690752
1541.046631	196038.823086	36.695770
1542.576037	196351.479068	36.700788
1543.984201	196676.763401	36.705805
1545.265229	197002.603568	36.710823
1547.124691	197324.921897	36.715840
1548.271063	197649.010066	36.720858
1549.702187	197976.848846	36.725876
1551.457865	198312.113551	36.730893
1552.881354	198651.408670	36.735911
1554.378073	198989.144454	36.740928
1555.878554	199336.974760	36.745946
1557.692778	199678.216412	36.750964
1559.187927	200023.397538	36.755981
1560.466467	200374.888178	36.760999
1561.867996	200720.621463	36.766016
1563.661910	201078.569146	36.771034
1565.228832	201426.170336	36.776052
1566.478484	201787.741154	36.781069
1568.168125	202133.128982	36.786087
1569.912059	202495.104162	36.791104
1571.450427	202867.869321	36.796122
1572.916973	203214.848156	36.801140
1574.865661	203584.374939	36.806157
1576.291630	203939.553414	36.811175
1578.078498	204301.314525	36.816192
1579.468952	204669.834260	36.821210
1581.328092	205036.653116	36.826228
1583.140615	205406.376415	36.831245
1584.406188	205770.516155	36.836263
1586.154453	206126.959437	36.841280
1587.532273	206496.010623	36.846298
1589.617093	206868.794086	36.851316
1591.294416	207227.311091	36.856333
1592.722890	207587.204074	36.861351
1594.955480	207947.257877	36.866368
1596.480242	208304.560541	36.871386
1597.757777	208667.848183	36.876404
1599.915744	209038.585296	36.881421
1601.180495	209397.548317	36.886439
1603.078626	209764.115909	36.891456
1604.591735	210116.895192	36.896474
1605.938987	210478.922143	36.901492
1607.787401	210841.350374	36.906509
1609.334013	211212.286980	36.911527
1610.990051	211558.394782	36.916544
1612.608083	211928.713147	36.921562
1614.237225	212295.145558	36.926580
1615.918509	212654.586769	36.931597
1617.692469	213020.566514	36.936615
1619.552416	213368.730280	36.941632
1620.890973	213739.407126	36.946650
1622.449250	214089.833043	36.951668
1624.699897	214457.416054	36.956685
1625.932548	214810.184259	36.961703
1627.583322	215169.818228	36.966720
1629.276025	215533.662640	36.971738
1630.837228	215878.075575	36.976756
1632.708158	216238.667739	36.981773
1633.974716	216605.532766	36.986791
1635.821079	216956.124915	36.991808
1637.603797	217315.211770	36.996826
1639.228831	217673.386248	37.001844
1640.741132	218018.144987	37.006861
1642.388392	218371.822809	37.011879
1643.829583	218698.740625	37.016896
1645.592234	219041.023241	37.021914
1646.944695	219369.024582	37.026932
1648.535091	219715.604833	37.031949
1650.145742	220059.744608	37.036967
1651.873376	220396.805315	37.041984
1653.148754	220751.822593	37.047002
1654.901179	221098.024996	37.052020
1656.476439	221454.874559	37.057037
1657.637593	221822.334317	37.062055
1659.362766	222177.866095	37.067072
1660.679364	222549.620431	37.072090
1661.825142	222923.740946	37.077108
1663.774675	223286.376360	37.082125
1665.069872	223674.393524	37.087143
1666.700095	224124.585683	37.092160
1668.330013	224523.167392	37.097178
1670.158197	224921.387477	37.102196
1672.086780	225301.786978	37.107213
1673.393672	225699.333719	37.112231
1675.322358	226098.252221	37.117248
1677.265510	226504.230831	37.122266
1678.744841	226894.158232	37.127284
1680.754140	227296.674003	37.132301
1682.293380	227691.343755	37.137319
1683.763056	228089.556835	37.142336
1685.289142	228498.582391	37.147354
1687.047351	228900.636481	37.152372
1688.985360	229310.612447	37.157389
1690.550799	229715.317011	37.162407
1692.242511	230125.310639	37.167424
1694.158379	230543.523693	37.172442
1695.696265	230956.059773	37.177460
1697.478823	231369.191613	37.182477
1698.906744	231791.883173	37.187495
1700.869646	232202.498195	37.192512
1702.354702	232623.607735	37.197530
1703.788699	233052.728239	37.202548
1706.064006	233474.903365	37.207565
1707.407944	233899.570361	37.212583
1709.637240	234323.457167	37.217600
1711.165837	234752.922113	37.222618
1712.652376	235172.793275	37.227636
1714.982781	235595.650464	37.232653
1716.554531	236031.741264	37.237671
1718.572429	236443.145090	37.242688
1719.957845	236878.659046	37.247706
1721.714102	237297.550715	37.252724
1723.583452	237722.876716	37.257741
1725.157908	238151.961043	37.262759
1727.015730	238582.117177	37.267776
1728.841727	239008.011919	37.272794
1730.565331	239434.127660	37.277812
1732.388327	239857.560602	37.282829
1733.988533	240285.959205	37.287847
1735.621511	240712.702066	37.292864
1737.772669	241137.810592	37.297882
1738.937044	241584.268487	37.302900
1741.279657	242003.682205	37.307917
1743.088122	242428.925827	37.312935
1744.781063	242849.972425	37.317952
1746.522809	243284.373401	37.322970
1747.939556	243705.822623	37.327988
1750.035412	244133.053739	37.333005
1751.568963	244559.921129	37.338023
1753.565958	244985.925113	37.343040
1755.270900	245407.354635	37.348058
1756.727049	245820.163467	37.353076
1758.857592	246215.079461	37.358093
1760.335355	246624.405557	37.363111
1762.271795	247018.109816	37.368128
1763.617482	247424.308710	37.373146
1765.339873	247839.794121	37.378164
1767.041783	248250.710834	37.383181
1768.447538	248671.279222	37.388199
1770.575226	249094.396120	37.393216
1772.310616	249515.800014	37.398234
1773.933916	249940.118766	37.403252
1775.747586	250359.554464	37.408269
1777.398055	250791.337985	37.413287
1779.405717	251207.541548	37.418304
1781.024770	251642.049074	37.423322
1783.073258	252066.858192	37.428340
1784.718005	252495.036695	37.433357
1786.105461	252930.599492	37.438375
1788.089948	253361.999430	37.443392
1790.223351	253810.268163	37.448410
1791.624634	254244.711664	37.453428
1793.687679	254685.092045	37.458445
1795.302074	255134.209224	37.463463
1796.971056	255578.414725	37.468480
1799.185260	256029.998890	37.473498
1800.756199	256478.895059	37.478516
1803.031507	256924.016927	37.483533
1804.430805	257377.006157	37.488551
1806.594982	257833.323973	37.493568
1808.607035	258277.193928	37.498586
1810.003463	258731.377701	37.503604
1811.818929	259176.575699	37.508621
1813.814016	259637.925907	37.513639
1815.672542	260091.499801	37.518656
1817.813257	260543.350398	37.523674
1819.143676	261011.033950	37.528692
1821.091733	261464.008482	37.533709
1823.242032	261923.427303	37.538727
1825.154294	262381.818326	37.543744
1826.784152	262835.886435	37.548762
1828.492342	263303.227284	37.553780
1830.615799	263756.959383	37.558797
1832.165723	264233.216970	37.563815
1833.786213	264688.631975	37.568832
1835.748758	265159.587727	37.573850
1837.753883	265625.074412	37.578868
1839.598462	266093.965853	37.583885
1841.620157	266560.388942	37.588903
1843.181426	267032.349306	37.593920
1844.984192	267499.772986	37.598938
1846.891252	267989.863871	37.603956
1848.751957	268447.166583	37.608973
1850.451895	268925.478196	37.613991
1852.083100	269399.456678	37.619008
1854.150074	269865.513100	37.624026
1856.150738	270353.604166	37.629044
1858.190142	270828.148435	37.634061
1860.035091	271310.726024	37.639079
1861.819980	271786.911310	37.644096
1863.694914	272257.187560	37.649114
1865.478486	272737.740841	37.654132
1867.444126	273214.046417	37.659149
1869.349383	273692.190139	37.664167
1871.281105	274179.295744	37.669184
1873.144259	274653.989943	37.674202
1874.843354	275137.474194	37.679220
1876.942589	275604.710088	37.684237
1878.861170	276073.753070	37.689255
1880.486235	276531.031510	37.694272
1882.672404	276977.344208	37.699290
1884.365879	277438.038809	37.704308
1886.003865	277883.703524	37.709325
1888.164180	278335.936393	37.714343
1889.667394	278799.606090	37.719360
1891.848517	279256.278841	37.724378
1893.451571	279713.681044	37.729396
1895.456096	280176.350257	37.734413
1897.310449	280643.107424	37.739431
1898.867725	281119.006288	37.744448
1900.921589	281582.959325	37.749466
1902.431146	282060.260664	37.754484
1904.707130	282546.604079	37.759501
1906.416733	283019.449860	37.764519
1908.192631	283510.750155	37.769536
1910.231276	283996.036284	37.774554
1911.918105	284474.825528	37.779572
1913.873737	284963.551580	37.784589
1916.087557	285464.806978	37.789607
1917.773397	285966.376516	37.794624
1919.486057	286454.883882	37.799642
1921.622021	286968.466513	37.804660
1923.254932	287468.032985	37.809677
1925.364186	287974.631208	37.814695
1927.218967	288489.143766	37.819712
1929.347191	288977.776996	37.824730
1931.160744	289497.372618	37.829748
1933.126863	290016.280597	37.834765
1935.309464	290523.161896	37.839783
1937.166624	291039.035733	37.844800
1939.896586	291556.058730	37.849818
1940.885892	292068.769625	37.854836
1943.407704	292578.355145	37.859853
1945.442052	293099.982207	37.864871
1947.192346	293617.183561	37.869888
1949.559262	294125.848211	37.874906
1951.133644	294653.513123	37.879924
1952.990752	295172.137596	37.884941
1955.021093	295681.460411	37.889959
1956.978213	296220.052495	37.894976
1959.247883	296730.905632	37.899994
1960.923290	297261.817797	37.905012
1963.278893	297787.128897	37.910029
1965.548925	298306.584448	37.915047
1967.278328	298834.381076	37.920064
1969.472473	299355.164532	37.925082
1971.320001	299874.326242	37.930100
1973.781450	300401.409585	37.935117
1975.573494	300924.816349	37.940135
1977.597377	301436.524497	37.945152
1979.894614	301953.518228	37.950170
1981.820305	302463.103655	37.955188
1983.468876	302986.014769	37.960205
1985.739918	303495.080339	37.965223
1987.629717	304012.256819	37.970240
1989.887492	304527.287033	37.975258
1991.578411	305048.960176	37.980276
1993.869597	305571.115229	37.985293
1996.070753	306084.698063	37.990311
1997.758488	306597.194377	37.995328
1999.659977	307115.391800	38.000346
2001.935364	307640.584335	38.005364
2003.645661	308148.623201	38.010381
2005.948956	308663.062275	38.015399
2008.046598	309176.744800	38.020416
2009.827971	309686.793971	38.025434
2011.596555	310200.117954	38.030452
2013.725800	310693.850413	38.035469
2015.667233	311183.699984	38.040487
2017.502526	311679.023813	38.045504
2019.776387	312168.075813	38.050522
2021.654572	312660.999132	38.055540
2023.348589	313158.698325	38.060557
2025.583939	313647.290004	38.065575
2027.234777	314151.008039	38.070592
2029.287593	314658.490676	38.075610
2031.533888	315160.503653	38.080628
2033.458265	315671.733219	38.085645
2035.296173	316183.354301	38.090663
2037.042720	316692.117385	38.095680
2039.417017	317211.514219	38.100698
2041.105508	317734.956228	38.105716
2043.482212	318259.042410	38.110733
2045.238712	318781.297175	38.115751
2047.260296	319316.733298	38.120768
2049.198269	319852.255133	38.125786
2051.445378	320394.526527	38.130804
2053.546393	320931.713950	38.135821
2055.712838	321468.048259	38.140839
2057.421842	322005.037644	38.145856
2059.683524	322546.095358	38.150874
2061.768174	323100.279137	38.155892
2063.593522	323645.639710	38.160909
2065.483504	324193.447692	38.165927
2067.630640	324749.637771	38.170944
2069.963085	325313.942256	38.175962
2071.783798	325876.345655	38.180980
2073.875725	326422.450110	38.185997
2076.324711	326987.456059	38.191015
2078.057035	327563.949021	38.196032
2080.142045	328128.674150	38.201050
2082.395680	328702.429526	38.206068
2084.228872	329268.708488	38.211085
2086.529263	329844.628182	38.216103
2088.593548	330428.679593	38.221120
2091.060653	330998.517941	38.226138
2092.802296	331586.621801	38.231156
2094.954715	332148.782849	38.236173
2097.256539	332734.268844	38.241191
2099.257924	333320.940572	38.246208
2101.595309	333896.660075	38.251226
2103.785823	334472.930797	38.256244
2105.659255	335053.537769	38.261261
2108.217439	335636.589249	38.266279
2109.991881	336206.106792	38.271296
2112.172086	336788.674854	38.276314
2114.508104	337372.530652	38.281332
2116.693471	337958.206977	38.286349
2119.269547	338530.282761	38.291367
2121.208243	339119.895561	38.296384
2123.247629	339688.214054	38.301402
2125.886468	340275.768669	38.306420
2127.484647	340855.670424	38.311437
2129.724789	341418.428126	38.316455
2131.262870	342012.743169	38.321472
2133.555320	342594.058113	38.326490
2135.705424	343194.298467	38.331508
2138.018691	343784.808974	38.336525
2140.616923	344358.640978	38.341543
2142.222786	344952.375592	38.346560
2144.255403	345542.174565	38.351578
2146.516971	346134.187095	38.356596
2148.269928	346721.454019	38.361613
2150.809990	347301.172941	38.366631
2152.913158	347894.762569	38.371648
2155.042368	348468.976635	38.376666
2156.805850	349028.676911	38.381684
2158.487651	349595.946227	38.386701
2160.805290	350148.917532	38.391719
2162.782860	350740.485610	38.396736
2164.976817	351308.511366	38.401754
2166.813971	351889.987326	38.406772
2168.714995	352476.748562	38.411789
2171.289139	353067.273211	38.416807
2173.012185	353656.179374	38.421824
2175.363244	354249.033755	38.426842
2177.710818	354850.380909	38.431860
2179.532837	355454.572048	38.436877
2181.880476	356060.291667	38.441895
2183.860335	356672.051331	38.446912
2185.916493	357286.275944	38.451930
2188.059123	357895.960818	38.456948
2190.112535	358521.635867	38.461965
2192.318549	359139.360108	38.466983
2194.690955	359767.754219	38.472000
2196.736373	360391.397363	38.477018
2199.234210	361027.717552	38.482036
2201.500654	361665.841666	38.487053
2203.597892	362300.000340	38.492071
2205.961606	362947.195410	38.497088
2208.308221	363587.152404	38.502106
2210.653455	364229.103184	38.507124
2212.684367	364874.773536	38.512141
2215.131314	365508.086357	38.517159
2217.177281	366157.715272	38.522176
2219.737311	366798.141484	38.527194
2221.999568	367440.305495	38.532212
2224.046624	368089.900871	38.537229
2226.362191	368737.056218	38.542247
2228.634122	369397.701670	38.547264
2231.123308	370053.023537	38.552282
2233.536449	370698.301975	38.557300
2235.479148	371351.940536	38.562317
2237.812688	372006.263651	38.567335
2240.226578	372666.750099	38.572352
2242.824208	373310.175860	38.577370
2245.199537	373963.923566	38.582388
2247.239318	374620.884714	38.587405
2249.518072	375266.153444	38.592423
2251.612534	375917.628607	38.597440
2254.065552	376565.431236	38.602458
2256.708389	377218.668021	38.607476
2259.103291	377878.044809	38.612493
2261.879106	378531.031706	38.617511
2263.606556	379173.680826	38.622528
2265.909683	379812.342987	38.627546
2268.522872	380458.954656	38.632564
2270.613417	381124.657494	38.637581
2272.759564	381769.697964	38.642599
2274.805318	382416.720138	38.647616
2277.030819	383078.152295	38.652634
2279.528270	383722.132949	38.657652
2281.616198	384389.722349	38.662669
2283.984885	385040.746478	38.667687
2286.295761	385691.640205	38.672704
2288.606573	386347.134854	38.677722
2291.028044	386993.547083	38.682740
2292.805787	387662.285585	38.687757
2295.445678	388312.386785	38.692775
2297.600028	388970.666758	38.697792
2300.005151	389634.088167	38.702810
2302.500953	390289.774232	38.707828
2304.534043	390951.023414	38.712845
2306.867401	391583.666693	38.717863
2308.974334	392204.927767	38.722880
2311.244566	392836.718988	38.727898
2313.876282	393460.934750	38.732916
2315.902568	394097.023454	38.737933
2318.129380	394716.514890	38.742951
2320.366386	395357.484417	38.747968
2322.504148	395991.942951	38.752986
2325.008849	396640.672009	38.758004
2327.167095	397286.656167	38.763021
2329.192655	397936.119948	38.768039
2331.474735	398597.209722	38.773056
2333.677554	399241.800063	38.778074
2336.072220	399906.997385	38.783092
2337.906298	400582.053273	38.788109
2340.325406	401247.772951	38.793127
2342.708525	401933.881169	38.798144
2344.899888	402614.303205	38.803162
2347.784807	403290.666961	38.808180
2349.691454	403989.776894	38.813197
2352.111787	404678.624482	38.818215
2354.305064	405373.446480	38.823232
2356.768107	406064.507513	38.828250
2359.613632	406761.872485	38.833268
2361.900220	407470.940382	38.838285
2364.345775	408163.876750	38.843303
2366.601371	408869.721263	38.848320
2368.922378	409575.105888	38.853338
2371.188050	410285.294149	38.858356
2373.533010	410994.867863	38.863373
2375.972446	411705.648264	38.868391
2378.414463	412419.702026	38.873408
2380.439696	413150.446335	38.878426
2383.124604	413858.645980	38.883444
2385.827299	414597.241847	38.888461
2388.243180	415313.880405	38.893479
2390.888456	416029.296268	38.898496
2393.145642	416756.633917	38.903514
2395.460325	417486.296646	38.908532
2397.893612	418220.831792	38.913549
2400.689991	418937.812770	38.918567
2402.936753	419668.335682	38.923584
2405.278637	420396.036309	38.928602
2407.822222	421123.657201	38.933620
2409.992793	421867.067632	38.938637
2412.842858	422590.290629	38.943655
2415.134564	423320.825770	38.948672
2417.701072	424058.332291	38.953690
2420.263251	424788.070241	38.958708
2422.400913	425530.362754	38.963725
2424.915251	426258.292354	38.968743
2427.619515	426994.320109	38.973760
2429.764336	427739.378880	38.978778
2432.522805	428468.669551	38.983796
2434.573488	429206.154747	38.988813
2437.224797	429954.098279	38.993831
2439.872206	430673.721060	38.998848
2441.981770	431427.680667	39.003866
2444.560072	432155.216871	39.008884
2446.992180	432904.469331	39.013901
2449.383530	433639.481360	39.018919
2452.359471	434385.559281	39.023936
2454.488942	435123.097984	39.028954
2457.261535	435844.210186	39.033972
2459.687811	436592.938763	39.038989
2461.734056	437326.472543	39.044007
2464.551773	438063.600113	39.049024
2466.950019	438796.572652	39.054042
2469.156735	439502.733503	39.059060
2471.600775	440210.958151	39.064077
2473.899354	440914.174948	39.069095
2476.509112	441625.565565	39.074112
2478.381604	442333.513202	39.079130
2480.849464	443048.473681	39.084148
2483.371213	443768.613028	39.089165
2486.000460	444492.353465	39.094183
2488.278808	445228.218611	39.099200
2490.118198	445956.795974	39.104218
2492.824512	446691.528974	39.109236
2495.220982	447438.327047	39.114253
2497.414153	448174.307960	39.119271
2499.993172	448931.342579	39.124288
2502.289840	449693.404119	39.129306
2504.895297	450448.407624	39.134324
2507.726524	451223.728662	39.139341
2509.935775	451989.413580	39.144359
2512.423353	452759.727683	39.149376
2515.119037	453542.975345	39.154394
2517.453082	454319.072460	39.159412
2520.027919	455094.038794	39.164429
2522.451483	455887.962343	39.169447
2524.838225	456676.703874	39.174464
2527.574299	457466.166229	39.179482
2530.094722	458263.318293	39.184500
2532.437340	459067.798897	39.189517
2534.968024	459862.661654	39.194535
2537.891507	460676.789513	39.199552
2540.308945	461488.591843	39.204570
2543.092999	462289.230607	39.209588
2545.606296	463112.526191	39.214605
2548.053144	463925.487503	39.219623
2550.963364	464728.887481	39.224640
2553.268623	465556.208921	39.229658
2556.066164	466371.638860	39.234676
2559.038496	467204.591961	39.239693
2561.151577	468029.211939	39.244711
2564.121914	468844.306996	39.249728
2566.456784	469673.923460	39.254746
2569.467536	470492.579746	39.259764
2572.221066	471313.011603	39.264781
2574.548813	472133.882377	39.269799
2577.570793	472942.276081	39.274816
2580.142119	473774.856866	39.279834
2582.575845	474593.127475	39.284852
2585.302326	475413.485988	39.289869
2587.711141	476238.709766	39.294887
2590.653403	477056.080928	39.299904
2593.172515	477887.981053	39.304922
2595.688449	478708.733111	39.309940
2598.406273	479530.627114	39.314957
2600.898104	480372.014229	39.319975
2603.374211	481185.136951	39.324992
2605.944807	482015.375882	39.330010
2608.530089	482845.473170	39.335028
2611.280458	483673.535730	39.340045
2613.691241	484515.298243	39.345063
2616.755732	485341.767465	39.350080
2619.050022	486187.811820	39.355098
2621.719127	487006.645641	39.360116
2624.406179	487837.250437	39.365133
2626.815325	488682.348431	39.370151
2629.627821	489514.872055	39.375168
2631.747571	490350.447982	39.380186
2635.021445	491188.064414	39.385204
2637.365893	492025.036593	39.390221
2640.197784	492849.574507	39.395239
2642.671705	493656.924471	39.400256
2645.210769	494462.863192	39.405274
2647.846209	495266.578270	39.410292
2650.253025	496062.068958	39.415309
2653.142685	496880.347862	39.420327
2655.792694	497669.517164	39.425344
2658.145140	498486.999417	39.430362
2660.387531	499299.365017	39.435380
2663.816588	500107.560845	39.440397
2665.822153	500931.941639	39.445415
2668.578525	501745.565763	39.450432
2671.111914	502574.468350	39.455450
2673.671224	503416.840769	39.460468
2676.456344	504248.088592	39.465485
2678.745036	505094.504151	39.470503
2681.431131	505941.919520	39.475520
2683.923149	506789.473924	39.480538
2686.728169	507645.352281	39.485556
2689.323164	508503.488565	39.490573
2691.588627	509381.395520	39.495591
2694.587422	510247.992543	39.500608
2696.973827	511132.437549	39.505626
2699.909238	512018.910193	39.510644
2702.954663	512896.343394	39.515661
2705.037815	513799.439127	39.520679
2708.469585	514684.470470	39.525696
2710.780988	515573.365721	39.530714
2713.463737	516472.227288	39.535732
2716.479166	517373.854130	39.540749
2718.810147	518291.664614	39.545767
2721.901100	519189.444611	39.550784
2724.319292	520109.500366	39.555802
2727.011541	521025.677463	39.560820
2729.833300	521947.067387	39.565837
2732.368288	522873.586533	39.570855
2735.163744	523800.308276	39.575872
2738.061268	524729.575223	39.580890
2740.982401	525651.377848	39.585908
2743.637305	526590.289278	39.590925
2746.320861	527533.215667	39.595943
2749.359162	528471.039030	39.600960
2751.935069	529409.433162	39.605978
2754.761630	530358.248414	39.610996
2757.679151	531297.271585	39.616013
2760.377166	532243.217526	39.621031
2763.402846	533193.679020	39.626048
2766.088387	534138.598076	39.631066
2768.974431	535077.534092	39.636084
2771.671334	536023.737479	39.641101
2774.341501	536984.426149	39.646119
2777.417131	537923.749245	39.651136
2779.707769	538894.335527	39.656154
2782.529046	539842.178238	39.661172
2785.706748	540800.664900	39.666189
2788.249160	541765.127395	39.671207
2791.110722	542709.300379	39.676224
2794.363970	543673.162793	39.681242
2796.854342	544629.641054	39.686260
2799.712788	545584.333442	39.691277
2802.689727	546547.891957	39.696295
2805.599220	547498.421245	39.701312
2808.217631	548469.497941	39.706330
2810.751123	549430.313838	39.711348
2813.887853	550382.315852	39.716365
2816.675406	551353.663141	39.721383
2819.632684	552306.716645	39.726400
2822.550665	553266.042844	39.731418
2825.169059	554211.227471	39.736436
2827.977616	555146.414021	39.741453
2830.464296	556073.146118	39.746471
2833.540412	556990.018794	39.751488
2836.099988	557921.484904	39.756506
2838.451238	558843.725843	39.761524
2841.425955	559767.206515	39.766541
2843.956683	560711.794616	39.771559
2846.464279	561657.926216	39.776576
2849.174073	562602.298787	39.781594
2851.702899	563567.526306	39.786612
2854.514212	564529.421719	39.791629
2856.997331	565510.683711	39.796647
2859.743723	566472.144551	39.801664
2862.709682	567465.279949	39.806682
2865.287972	568465.983614	39.811700
2868.229367	569452.392596	39.816717
2870.532363	570469.752275	39.821735
2873.500475	571487.422979	39.826752
2876.675874	572505.279062	39.831770
2879.382210	573534.070964	39.836788
2882.217904	574550.162159	39.841805
2884.926420	575604.878570	39.846823
2887.949415	576639.535751	39.851840
2890.822096	577688.480118	39.856858
2893.850670	578745.888381	39.861876
2896.822381	579793.484764	39.866893
2899.678172	580848.685209	39.871911
2903.079085	581912.080561	39.876928
2906.088228	582967.876098	39.881946
2908.601872	584042.064467	39.886964
2911.679391	585080.968362	39.891981
2914.905218	586154.802484	39.896999
2918.138750	587226.334293	39.902016
2921.414018	588294.154955	39.907034
2924.433347	589365.030350	39.912052
2927.576828	590415.743053	39.917069
2930.558453	591482.926731	39.922087
2933.705295	592545.327412	39.927104
2936.832400	593604.629926	39.932122
2939.590848	594665.651630	39.937140
2942.907465	595723.580220	39.942157
2946.038829	596782.445708	39.947175
2949.055605	597836.626399	39.952192
2952.442196	598903.020490	39.957210
2954.398420	599970.704221	39.962228
2957.597342	601025.366614	39.967245
2960.860688	602090.986578	39.972263
2963.635968	603158.790948	39.977280
2966.918001	604213.697828	39.982298
2969.856670	605285.481533	39.987316
2972.987342	606341.667999	39.992333
2975.801949	607413.771926	39.997351
2978.696736	608482.208307	40.002368
2982.127404	609545.001435	40.007386
2984.683969	610612.340716	40.012404
2988.124284	611663.024759	40.017421
2990.951295	612732.268116	40.022439
2994.157092	613799.295698	40.027456
2997.215569	614860.193766	40.032474
3000.088822	615925.771016	40.037492
3003.232167	616986.100727	40.042509
3006.319719	618053.936528	40.047527
3009.261592	619117.193106	40.052544
3012.435353	620168.961230	40.057562
3015.218707	621245.882178	40.062580
3018.483939	622292.781422	40.067597
3021.399799	623365.821500	40.072615
3024.150610	624413.249533	40.077632
3027.287105	625438.379222	40.082650
3030.118949	626461.163054	40.087668
3033.196293	627485.007305	40.092685
3036.292610	628506.852016	40.097703
3038.792597	629524.002163	40.102720
3041.976435	630542.739572	40.107738
3044.582685	631588.137584	40.112756
3047.766202	632609.521353	40.117773
3050.888633	633660.219927	40.122791
3053.180413	634701.515551	40.127808
3056.547467	635752.811847	40.132826
3059.125589	636806.028356	40.137844
3062.394112	637855.431095	40.142861
3065.264654	638927.645639	40.147879
3067.940936	640005.917292	40.152896
3071.193671	641088.021515	40.157914
3073.882274	642189.408324	40.162932
3076.962085	643281.584328	40.167949
3079.998162	644386.516837	40.172967
3082.692620	645498.166917	40.177984
3086.232470	646609.854596	40.183002
3089.012823	647741.536200	40.188020
3092.183310	648862.607816	40.193037
3095.329768	650008.180084	40.198055
3097.839362	651139.622144	40.203072
3101.521878	652275.775195	40.208090
3104.229265	653439.711539	40.213108
3107.449662	654577.869038	40.218125
3110.561651	655747.146137	40.223143
3113.751039	656909.447730	40.228160
3117.118300	658070.187658	40.233178
3120.054690	659245.201812	40.238196
3123.370248	660418.219209	40.243213
3126.563109	661604.506818	40.248231
3129.582746	662773.504238	40.253248
3132.957358	663954.445651	40.258266
3135.891040	665151.836705	40.263284
3139.013306	666331.133750	40.268301
3142.674458	667518.455311	40.273319
3145.452615	668716.469841	40.278336
3148.891228	669909.648134	40.283354
3151.918719	671100.058014	40.288372
3155.115103	672294.765254	40.293389
3158.282659	673504.987619	40.298407
3160.850989	674700.237906	40.303424
3164.430672	675917.636811	40.308442
3167.852921	677131.820897	40.313460
3171.016254	678333.315773	40.318477
3174.153237	679545.590514	40.323495
3177.309447	680759.739667	40.328512
3180.667020	681971.310772	40.333530
3183.596994	683183.487487	40.338548
3186.987119	684400.940029	40.343565
3190.037950	685619.477411	40.348583
3193.295864	686854.102036	40.353600
3196.893635	688073.410766	40.358618
3199.834457	689289.237997	40.363636
3202.862158	690516.301174	40.368653
3206.262937	691735.939574	40.373671
3209.478438	692972.360875	40.378688
3212.891143	694192.405548	40.383706
3215.704215	695421.210476	40.388724
3219.140507	696637.640869	40.393741
3222.457337	697864.782990	40.398759
3225.287884	699099.965312	40.403776
3228.871942	700312.441866	40.408794
3232.020456	701551.043067	40.413812
3235.387775	702757.812654	40.418829
3238.558310	703949.630488	40.423847
3241.578348	705127.584630	40.428864
3244.778302	706306.289661	40.433882
3247.860713	707478.116135	40.438900
3251.179187	708661.927220	40.443917
3254.081181	709849.703777	40.448935
3257.282165	711050.089481	40.453952
3260.682115	712252.005699	40.458970
3263.576848	713439.727748	40.463988
3266.956088	714649.523854	40.469005
3270.083038	715846.420945	40.474023
3273.056960	717070.979131	40.479040
3276.420973	718285.350630	40.484058
3279.335084	719526.577040	40.489076
3282.507632	720751.156736	40.494093
3285.610117	721991.885321	40.499111
3288.929872	723248.757050	40.504128
3292.440968	724496.656238	40.509146
3295.307710	725764.341466	40.514164
3298.876693	727026.971017	40.519181
3302.139203	728292.025506	40.524199
3305.148958	729571.153332	40.529216
3308.873168	730852.827073	40.534234
3312.132498	732136.103275	40.539252
3315.179478	733412.890162	40.544269
3319.015856	734710.870401	40.549287
3322.077909	736028.859169	40.554304
3325.712243	737304.239489	40.559322
3328.816260	738612.269824	40.564340
3332.239680	739912.631669	40.569357
3335.728352	741223.622336	40.574375
3338.686079	742547.652243	40.579392
3342.503774	743867.175669	40.584410
3345.518163	745195.435631	40.589428
3348.963756	746512.356696	40.594445
3352.637445	747837.643699	40.599463
3355.780566	749178.907305	40.604480
3359.348543	750499.618240	40.609498
3362.644860	751841.775277	40.614516
3365.965478	753169.706293	40.619533
3369.710843	754516.691902	40.624551
3372.902427	755850.287035	40.629568
3376.402433	757189.407677	40.634586
3379.899946	758531.148120	40.639604
3383.372985	759877.232243	40.644621
3387.029144	761206.465365	40.649639
3390.456479	762548.833806	40.654656
3393.939763	763883.083824	40.659674
3397.329877	765228.078340	40.664692
3400.557188	766573.398634	40.669709
3404.220023	767921.255646	40.674727
3407.688653	769255.482184	40.679744
3411.046095	770604.622371	40.684762
3414.539552	771957.522619	40.689780
3418.322831	773296.077289	40.694797
3421.886278	774637.665697	40.699815
3425.173607	775979.299251	40.704832
3428.393524	777314.756622	40.709850
3432.020084	778664.382676	40.714868
3435.193879	780004.850919	40.719885
3438.655419	781347.182369	40.724903
3442.675564	782706.686290	40.729920
3446.031607	784044.362122	40.734938
3449.512961	785394.567502	40.739956
3452.943658	786735.357089	40.744973
3456.671590	788074.766879	40.749991
3459.965681	789421.200614	40.755008
3463.372226	790726.373886	40.760013
3467.301710	792011.244068	40.765018
3470.380422	793235.906485	40.770023
3473.608066	794374.152839	40.775028
3476.730151	795482.380846	40.780032
3479.885038	796512.277574	40.785037
3483.183531	797476.571494	40.790042
3485.987778	798371.026829	40.795047
3489.047914	799181.610654	40.800052
3491.308847	799922.853133	40.805056
3494.001758	800608.016183	40.810061
3496.668112	801230.274972	40.815066
3498.625156	801782.793500	40.820071
3500.612025	802267.624858	40.825076
3502.261787	802689.355964	40.830080
3504.751092	803069.873952	40.835085
3506.587442	803386.333346	40.840090
3508.436881	803658.494034	40.845095
3510.019104	803866.155052	40.850100
3511.007533	804043.211069	40.855104
3512.857550	804167.898242	40.860109
3514.289281	804256.072349	40.865114
3515.263130	804300.091984	40.870119
3516.611289	804305.852103	40.875124
3517.459283	804294.924911	40.880128
3517.949212	804223.498962	40.885133
3519.142730	804140.187860	40.890138
3519.450530	804012.496843	40.895143
3520.742585	803867.772457	40.900148
3521.305150	803703.942144	40.905152
3521.927538	803511.213631	40.910157
3522.456281	803303.243293	40.915162
3522.768659	803072.252129	40.920167
3523.318357	802832.533198	40.925172
3523.634895	802568.124883	40.930176
3523.898970	802282.918465	40.935181
3524.227831	802007.352547	40.940186
3524.621408	801705.276515	40.945191
3525.056367	801395.380708	40.950196
3524.957106	801082.468409	40.955200
3525.402687	800736.876642	40.960205
3526.118382	800412.908513	40.965210
3525.663343	800059.532314	40.970215
3525.554539	799696.071360	40.975220
3525.825648	799337.484770	40.980224
3525.978768	798967.219913	40.985229
3526.103158	798596.056689	40.990234
3526.234073	798234.933421	40.995239
3526.162766	797841.775462	41.000244
3526.334013	797446.984667	41.005248
3526.342689	797055.143416	41.010253
3526.297571	796662.159960	41.015258
3526.193451	796269.065900	41.020263
3526.187221	795874.657130	41.025268
3526.476657	795475.562286	41.030272
3526.244967	795071.915168	41.035277
3526.229319	794667.276225	41.040282
3526.211195	794256.918102	41.045287
3526.027041	793841.357845	41.050292
3525.780836	793440.762082	41.055296
3525.619511	793037.329994	41.060301
3526.006538	792623.322548	41.065306
3525.820283	792222.058058	41.070311
3525.701873	791816.977103	41.075316
3525.493342	791410.266585	41.080320
3525.320571	790988.247892	41.085325
3525.360659	790590.636139	41.090330
3525.249148	790192.093457	41.095335
3525.340927	789772.022171	41.100340
3524.988126	789367.330724	41.105344
3524.756181	788965.397355	41.110349
3524.755874	788556.473600	41.115354
3524.442069	788159.668304	41.120359
3524.981606	787756.310682	41.125364
3524.384453	787355.673449	41.130368
3524.291909	786959.108785	41.135373
3524.086116	786552.512307	41.140378
3523.400419	786165.832996	41.145383
3523.977083	785761.422268	41.150388
3523.630466	785382.658449	41.155392
3523.661471	784985.422923	41.160397
3523.362899	784598.545839	41.165402
3523.092126	784219.855486	41.170407
3523.049377	783824.288833	41.175412
3522.530592	783445.401731	41.180416
3522.520536	783059.426851	41.185421
3522.377536	782694.897987	41.190426
3522.043902	782327.184847	41.195431
3521.965515	781950.015500	41.200436
3521.768432	781582.832136	41.205440
3522.049329	781207.778437	41.210445
3521.989713	780844.962461	41.215450
3521.323799	780482.572557	41.220455
3521.471840	780112.502320	41.225460
3521.074095	779758.642454	41.230464
3521.009837	779400.576890	41.235469
3521.011826	779031.311989	41.240474
3520.486881	778706.209638	41.245479
3520.680075	778351.347084	41.250484
3520.477802	778010.657706	41.255488
3520.203339	777653.918672	41.260493
3520.702325	777308.060434	41.265498
3520.001358	776959.282349	41.270503
3519.910603	776617.524882	41.275508
3519.783222	776291.412216	41.280512
3519.578772	775941.617509	41.285517
3519.430314	775609.225473	41.290522
3519.065555	775282.171407	41.295527
3519.204342	774957.481636	41.300532
3518.977287	774637.367819	41.305536
3518.688931	774308.878943	41.310541
3518.682309	773988.601975	41.315546
3518.223401	773678.776541	41.320551
3518.324681	773365.841568	41.325556
3518.001512	773047.644130	41.330560
3518.152927	772734.526259	41.335565
3518.085048	772428.671651	41.340570
3517.707668	772127.288441	41.345575
3517.593323	771821.613297	41.350580
3517.494159	771520.701279	41.355584
3517.318093	771215.454521	41.360589
3517.393676	770915.326491	41.365594
3517.101191	770625.445152	41.370599
3517.153357	770321.601851	41.375604
3516.543143	770033.966763	41.380608
3516.358914	769755.464287	41.385613
3516.792711	769469.162687	41.390618
3516.339489	769189.944152	41.395623
3516.388592	768902.501420	41.400628
3515.820012	768619.732382	41.405632
3515.983815	768341.415128	41.410637
3515.825200	768074.081581	41.415642
3515.560826	767811.191543	41.420647
3515.668638	767532.458945	41.425652
3515.315307	767273.704709	41.430656
3515.106831	766995.694174	41.435661
3515.203085	766736.107823	41.440666
3514.907221	766485.006374	41.445671
3515.157676	766207.679551	41.450676
3514.834440	765954.938003	41.455680
3514.600812	765709.814549	41.460685
3514.757381	765451.603279	41.465690
3514.202121	765198.972991	41.470695
3514.476809	764952.212563	41.475700
3513.900284	764709.923186	41.480704
3513.719738	764466.032187	41.485709
3513.697393	764220.874454	41.490714
3513.513691	763994.177525	41.495719
3513.451098	763753.498422	41.500724
3513.243882	763530.095271	41.505728
3513.015290	763293.028663	41.510733
3513.188707	763067.428479	41.515738
3512.959563	762847.855366	41.520743
3512.901820	762623.019714	41.525748
3512.741875	762399.525857	41.530752
3512.472642	762183.540411	41.535757
3512.777834	761953.594067	41.540762
3512.363541	761747.386185	41.545767
3512.242246	761521.837584	41.550772
3512.143997	761316.897685	41.555776
3512.069581	761117.325220	41.560781
3511.936198	760893.437040	41.565786
3511.986744	760696.250082	41.570791
3511.837120	760480.640174	41.575796
3511.538732	760286.953395	41.580800
3511.567860	760089.556809	41.585805
3511.927705	759884.255912	41.590810
3511.816970	759686.477165	41.595815
3511.738974	759484.493945	41.600820
3511.290018	759286.069712	41.605824
3511.101248	759075.557764	41.610829
3511.234326	758886.254283	41.615834
3510.702828	758712.303275	41.620839
3510.852655	758512.970640	41.625844
3510.591205	758327.665962	41.630848
3510.572480	758136.148154	41.635853
3510.819164	757960.225794	41.640858
3510.401183	757778.239974	41.645863
3510.302995	757593.137254	41.650868
3510.340810	757419.161553	41.655872
3510.064739	757245.233596	41.660877
3510.461074	757064.330408	41.665882
3510.002374	756891.460942	41.670887
3510.283311	756717.527883	41.675892
3509.948076	756549.961012	41.680896
3509.666168	756380.308540	41.685901
3509.918181	756199.902246	41.690906
3509.723679	756029.437793	41.695911
3510.121417	755864.696871	41.700916
3509.659495	755710.756821	41.705920
3509.694241	755535.553937	41.710925
3509.881786	755370.195244	41.715930
3509.486557	755202.411238	41.720935
3509.498885	755023.942051	41.725940
3509.098691	754873.480186	41.730944
3508.747042	754720.341330	41.735949
3508.968263	754565.031396	41.740954
3508.998821	754421.648630	41.745959
3509.160048	754260.565777	41.750964
3508.838241	754116.099757	41.755968
3509.020899	753963.697129	41.760973
3509.096850	753808.692083	41.765978
3508.615809	753658.910985	41.770983
3508.869757	753501.697790	41.775988
3508.791646	753359.991988	41.780992
3508.551166	753216.088195	41.785997
3508.586279	753052.087323	41.791002
3508.443245	752914.038253	41.796007
3508.446998	752768.159915	41.801012
3508.252818	752620.731122	41.806016
3508.180715	752482.662629	41.811021
3507.930095	752348.571981	41.816026
3507.753016	752215.405236	41.821031
3508.001663	752077.326021	41.826036
3508.070723	751933.742364	41.831040
3507.676931	751806.580327	41.836045
3507.551936	751672.556002	41.841050
3507.331262	751540.125641	41.846055
3507.502736	751408.912595	41.851060
3507.671128	751293.799978	41.856064
3507.390366	751167.497863	41.861069
3507.807103	751036.336869	41.866074
3507.157349	750919.130715	41.871079
3507.374459	750793.234405	41.876084
3507.294505	750675.881281	41.881088
3507.482930	750547.071271	41.886093
3507.465002	750409.549555	41.891098
3507.172744	750298.054725	41.896103
3507.257352	750163.574509	41.901108
3507.318602	750054.685543	41.906112
3507.017032	749936.073295	41.911117
3507.321365	749819.434302	41.916122
3506.805734	749702.484030	41.921127
3507.170843	749581.286346	41.926132
3506.806413	749459.614118	41.931136
3506.713492	749341.007792	41.936141
3507.064826	749231.861856	41.941146
3506.686636	749135.285114	41.946151
3506.664846	749005.248957	41.951156
3506.385864	748904.996838	41.956160
3506.646892	748791.264621	41.961165
3506.499145	748673.101809	41.966170
3506.112655	748566.242122	41.971175
3506.285582	748459.931136	41.976180
3506.134178	748358.415666	41.981184
3506.047131	748262.916577	41.986189
3506.064627	748155.984688	41.991194
3506.117919	748060.459991	41.996199
3506.300647	747958.241869	42.001204
3506.035526	747852.340661	42.006208
3506.163998	747744.149457	42.011213
3506.517319	747651.584665	42.016218
3506.300736	747551.502483	42.021223
3506.413725	747446.521796	42.026228
3506.199693	747349.105140	42.031232
3505.880881	747242.907986	42.036237
3506.040557	747141.325395	42.041242
3505.700113	747044.716476	42.046247
3506.002815	746947.852128	42.051252
3505.903528	746846.407210	42.056256
3505.511156	746759.242780	42.061261
3505.698480	746672.920887	42.066266
3505.488676	746574.653682	42.071271
3505.290771	746480.238325	42.076276
3505.458338	746388.578791	42.081280
3505.489759	746306.924420	42.086285
3505.662113	746211.604590	42.091290
3505.394343	746128.663170	42.096295
3505.547849	746036.754699	42.101300
3505.378685	745951.373254	42.106304
3505.178177	745862.536113	42.111309
3505.464905	745768.971438	42.116314
3505.108590	745692.169065	42.121319
3505.149254	745603.042097	42.126324
3505.185032	745523.603147	42.131328
3505.241315	745450.981376	42.136333
3505.519485	745352.420689	42.141338
3505.038396	745272.965498	42.146343
3505.169034	745185.005300	42.151348
3505.144575	745116.496575	42.156352
3504.954778	745023.841867	42.161357
3505.247323	744935.506164	42.166362
3504.766621	744862.324783	42.171367
3504.858535	744779.804144	42.176372
3504.851744	744704.120916	42.181376
3504.793037	744624.144635	42.186381
3505.162421	744541.526338	42.191386
3504.955778	744473.091447	42.196391
3505.043527	744390.023598	42.201396
3504.906444	744304.371735	42.206400
3504.561750	744240.011421	42.211405
3505.084978	744155.188451	42.216410
3504.945734	744078.037862	42.221415
3504.753977	744002.724421	42.226420
3504.494000	743931.821635	42.231424
3504.319180	743850.768937	42.236429
3504.647028	743778.828551	42.241434
3504.450971	743707.418801	42.246439
3504.533765	743631.858805	42.251444
3504.491527	743563.833877	42.256448
3504.317875	743486.238170	42.261453
3504.355329	743424.181447	42.266458
3504.307345	743369.109816	42.271463
3504.401077	743297.549710	42.276468
3504.197930	743226.433424	42.281472
3504.280407	743166.048349	42.286477
3504.174616	743090.464784	42.291482
3503.939529	743036.064437	42.296487
3504.383580	742968.003680	42.301492
3504.275756	742900.725516	42.306496
3504.038412	742836.682148	42.311501
3504.334147	742769.633050	42.316506
3504.026831	742707.429700	42.321511
3504.265351	742639.548317	42.326516
3504.262310	742578.431114	42.331520
3503.947262	742518.798856	42.336525
3504.122079	742451.420837	42.341530
3503.977276	742405.555935	42.346535
3503.983150	742337.463040	42.351540
3504.126144	742271.275521	42.356544
3503.899031	742216.225347	42.361549
3504.121107	742154.968870	42.366554
3504.061916	742090.098869	42.371559
3503.729910	742022.850152	42.376564
3503.909590	741971.291764	42.381568
3503.873474	741894.646764	42.386573
3504.171696	741842.771291	42.391578
3503.994960	741782.912868	42.396583
3503.818837	741718.207437	42.401588
3504.036904	741672.822477	42.406592
3503.883274	741613.552410	42.411597
3503.936559	741550.044160	42.416602
3503.906025	741494.659836	42.421607
3504.345343	741420.701382	42.426612
3504.037654	741369.516107	42.431616
3503.657266	741311.566988	42.436621
3503.699947	741237.672177	42.441626
3503.665734	741193.414081	42.446631
3503.823107	741134.831034	42.451636
3503.675844	741079.957612	42.456640
3503.502672	741016.334017	42.461645
3503.814862	740964.846153	42.466650
3503.725375	740921.386975	42.471655
3503.940808	740863.336398	42.476660
3503.783583	740803.961938	42.481664
3503.791227	740747.230690	42.486669
3503.265018	740688.806436	42.491674
3503.211796	740637.426113	42.496679
3503.321413	740596.009678	42.501684
3503.473035	740542.220875	42.506688
3503.399254	740503.702912	42.511693
3503.310882	740444.512256	42.516698
3503.346901	740405.530569	42.521703
3503.338510	740346.969010	42.526708
3503.263664	740304.839515	42.531712
3503.106759	740253.473787	42.536717
3503.484944	740195.391502	42.541722
3503.230328	740162.095301	42.546727
3503.661983	740112.808071	42.551732
3503.494763	740061.393334	42.556736
3503.268344	740011.175160	42.561741
3503.429683	739963.563865	42.566746
3503.192624	739918.689030	42.571751
3503.405114	739854.646306	42.576756
3503.296753	739812.025063	42.581760
3503.378680	739762.595423	42.586765
3503.542098	739717.059872	42.591770
3502.991951	739664.864735	42.596775
3503.412614	739622.105839	42.601780
3503.403961	739576.350500	42.606784
3503.466802	739525.141715	42.611789
3503.739659	739464.993820	42.616794
3503.455309	739424.823412	42.621799
3503.421865	739362.746495	42.626804
3503.470591	739315.941367	42.631808
3503.381758	739274.105517	42.636813
3503.629407	739211.981106	42.641818
3503.218878	739182.070388	42.646823
3503.422241	739126.630980	42.651828
3503.458661	739076.264643	42.656832
3503.174548	739028.226440	42.661837
3503.336184	738975.266372	42.666842
3503.145332	738935.820145	42.671847
3503.401745	738890.462421	42.676852
3503.131703	738840.046142	42.681856
3503.118559	738795.870139	42.686861
3503.194044	738748.364656	42.691866
3503.188825	738712.102421	42.696871
3503.330441	738663.348725	42.701876
3503.453996	738607.671489	42.706880
3503.160263	738564.084636	42.711885
3503.539096	738510.244641	42.716890
3503.264830	738468.187736	42.721895
3503.263544	738430.538302	42.726900
3503.497611	738375.929667	42.731904
3503.241818	738330.702627	42.736909
3503.405873	738265.912974	42.741914
3502.860630	738248.092857	42.746919
3503.149496	738197.976220	42.751924
3503.051991	738147.725026	42.756928
3503.202213	738106.833166	42.761933
3503.632730	738054.366909	42.766938
3503.082476	738013.441558	42.771943
3503.285785	737975.063587	42.776948
3503.481209	737914.669357	42.781952
3503.367376	737879.361296	42.786957
3503.323260	737830.187810	42.791962
3503.272782	737781.509849	42.796967
3503.056192	737721.627349	42.801972
3503.164877	737680.641191	42.806977
3503.167147	737651.646271	42.811981
3503.237345	737595.822323	42.816986
3503.295844	737558.703193	42.821991
3503.365944	737512.824058	42.826996
3503.199790	737465.350743	42.832001
3503.218221	737416.114919	42.837005
3503.111053	737365.810910	42.842010
3503.493306	737318.543246	42.847015
3503.363327	737272.101923	42.852020
3503.297651	737227.183663	42.857025
3503.471483	737187.421280	42.862029
3503.304207	737127.278783	42.867034
3503.397439	737086.193158	42.872039
3503.391357	737037.849725	42.877044
3503.175312	736985.631433	42.882049
3502.944172	736940.936759	42.887053
3503.553581	736892.392065	42.892058
3502.969314	736850.427185	42.897063
3502.903463	736810.999326	42.902068
3502.838874	736768.354578	42.907073
3502.808539	736727.040044	42.912077
3503.142755	736687.892052	42.917082
3503.105123	736651.427850	42.922087
3502.961790	736597.463060	42.927092
3503.057937	736560.778460	42.932097
3502.992055	736521.398664	42.937101
3502.958572	736475.382183	42.942106
3502.958442	736439.900562	42.947111
3503.056994	736396.633114	42.952116
3503.106300	736355.155077	42.957121
3503.068500	736315.027333	42.962125
3502.973466	736268.871345	42.967130
3502.784160	736236.884119	42.972135
3503.154351	736188.622018	42.977140
3502.988346	736147.128892	42.982145
3502.685519	736111.448249	42.987149
3502.863247	736064.800745	42.992154
3502.805492	736030.415557	42.997159
3502.592920	735993.185356	43.002164
3502.523616	735961.276234	43.007169
3502.786953	735930.895843	43.012173
3503.027762	735892.848129	43.017178
3503.175899	735858.378788	43.022183
3502.866034	735805.277426	43.027188
3503.050078	735773.226830	43.032193
3502.829969	735738.273253	43.037197
3502.604185	735689.710421	43.042202
3502.791275	735647.166703	43.047207
3502.807491	735607.818377	43.052212
3502.970320	735574.929128	43.057217
3502.745456	735538.688675	43.062221
3502.784967	735492.456552	43.067226
3502.747502	735459.005922	43.072231
3502.871559	735412.363466	43.077236
3502.778160	735381.693327	43.082241
3502.819734	735344.418235	43.087245
3503.091187	735303.046630	43.092250
3503.052214	735267.962168	43.097255
3503.004325	735230.057868	43.102260
3502.842297	735182.867290	43.107265
3503.050485	735150.810231	43.112269
3503.004125	735111.568771	43.117274
3502.950841	735076.287850	43.122279
3502.848262	735027.849193	43.127284
3503.044413	734992.477309	43.132289
3502.576968	734961.619717	43.137293
3502.924241	734916.075998	43.142298
3502.778850	734874.374902	43.147303
3503.115152	734841.206585	43.152308
3502.826866	734799.825624	43.157313
3502.748244	734767.665805	43.162317
3502.863236	734724.634113	43.167322
3502.829987	734686.427852	43.172327
3502.762401	734643.425808	43.177332
3502.527268	734601.193607	43.182337
3502.768932	734575.563449	43.187341
3502.777668	734527.301423	43.192346
3502.764843	734501.910956	43.197351
3502.844244	734454.676318	43.202356
3502.791420	734415.432521	43.207361
3502.522499	734392.063862	43.212365
3503.084132	734359.400921	43.217370
3502.736980	734322.630633	43.222375
3502.551724	734290.387474	43.227380
3502.637287	734256.020567	43.232385
3502.364191	734216.119093	43.237389
3502.814183	734188.671372	43.242394
3502.800075	734150.855415	43.247399
3502.665672	734116.672658	43.252404
3502.880939	734077.482041	43.257409
3502.836998	734044.373094	43.262413
3503.010313	733993.308678	43.267418
3502.871363	733963.729662	43.272423
3502.860928	733921.654874	43.277428
3502.976835	733883.766737	43.282433
3502.433366	733842.373389	43.287437
3503.042833	733812.670501	43.292442
3502.776296	733771.973700	43.297447
3502.655168	733735.311990	43.302452
3502.935454	733679.574665	43.307457
3502.505979	733649.646337	43.312461
3502.667447	733616.204762	43.317466
3502.777880	733579.751709	43.322471
3502.557483	733553.402369	43.327476
3502.707829	733510.358359	43.332481
3502.572441	733480.281935	43.337485
3502.600508	733439.633920	43.342490
3502.669537	733418.236446	43.347495
3502.595776	733375.773200	43.352500
3502.910465	733348.245906	43.357505
3502.601816	733311.266625	43.362509
3502.664556	733269.027854	43.367514
3502.367872	733241.353400	43.372519
3502.590913	733205.078124	43.377524
3502.635255	733172.099564	43.382529
3502.554214	733141.319827	43.387533
3502.853325	733092.654809	43.392538
3502.705659	733076.935939	43.397543
3502.641578	733023.726182	43.402548
3502.965749	732984.116247	43.407553
3502.791490	732953.499676	43.412557
3502.880161	732916.057051	43.417562
3502.737778	732887.761861	43.422567
3502.671282	732848.661207	43.427572
3502.875605	732805.802580	43.432577
3502.576045	732770.403602	43.437581
3502.547672	732741.792059	43.442586
3502.692143	732714.835255	43.447591
3502.452823	732676.009788	43.452596
3502.756499	732649.818689	43.457601
3502.452467	732623.480088	43.462605
3502.633502	732571.167648	43.467610
3502.503848	732550.691796	43.472615
3502.785226	732516.483252	43.477620
3502.539008	732479.291824	43.482625
3502.385690	732439.807409	43.487629
3502.469151	732401.769126	43.492634
3502.393471	732379.848119	43.497639
3502.454485	732347.408070	43.502644
3502.717108	732306.022535	43.507649
3502.476938	732287.099093	43.512653
3502.860719	732238.811079	43.517658
3502.665832	732214.631700	43.522663
3502.611113	732180.873215	43.527668
3502.913835	732141.757816	43.532673
3502.351404	732103.626502	43.537677
3502.451651	732069.544939	43.542682
3502.243136	732036.950001	43.547687
3501.906056	732010.070193	43.552692
3502.248992	731976.641443	43.557697
3502.028043	731952.762657	43.562701
3502.416945	731933.289106	43.567706
3502.397791	731919.774943	43.572711
3502.359465	731892.201831	43.577716
3502.540533	731844.737099	43.582721
3502.322290	731831.453651	43.587725
3502.517906	731779.579321	43.592730
3502.200432	731761.855748	43.597735
3502.346035	731731.875052	43.602740
3502.829961	731696.441300	43.607745
3502.379688	731668.638209	43.612749
3502.568369	731628.251709	43.617754
3502.506271	731607.960400	43.622759
3502.581604	731577.990714	43.627764
3502.374417	731529.993913	43.632769
3502.403431	731516.322590	43.637773
3502.724138	731473.140626	43.642778
3502.760689	731448.376133	43.647783
3502.482528	731409.947117	43.652788
3502.870815	731381.608730	43.657793
3502.440492	731341.867488	43.662797
3502.537605	731307.634682	43.667802
3502.215840	731278.125460	43.672807
3502.415597	731242.835586	43.677812
3502.435513	731214.210681	43.682817
3502.304713	731193.186875	43.687821
3502.363244	731154.057424	43.692826
3502.391845	731130.234128	43.697831
3502.263647	731105.594771	43.702836
3502.363320	731073.687958	43.707841
3502.474762	731056.932073	43.712845
3502.239615	731021.910974	43.717850
3502.115856	731000.340789	43.722855
3502.168816	730962.795969	43.727860
3502.335701	730935.185785	43.732865
3502.350109	730911.314665	43.737869
3502.383140	730884.370129	43.742874
3502.161283	730855.338109	43.747879
3502.045650	730823.416267	43.752884
3502.415246	730789.433502	43.757889
3502.631884	730764.488683	43.762893
3502.370476	730733.333326	43.767898
3502.650412	730703.920954	43.772903
3502.515842	730685.669666	43.777908
3502.462901	730646.605656	43.782913
3502.580211	730615.734099	43.787917
3502.535895	730583.849086	43.792922
3502.639913	730551.889984	43.797927
3502.013031	730518.020751	43.802932
3502.762629	730488.579736	43.807937
3502.428796	730457.435252	43.812941
3502.219635	730420.921578	43.817946
3502.712201	730390.680663	43.822951
3502.313060	730361.824657	43.827956
3502.668372	730337.400440	43.832961
3502.341953	730306.452249	43.837965
3502.658818	730272.030293	43.842970
3502.427755	730249.435780	43.847975
3502.103562	730220.665971	43.852980
3502.533420	730192.366112	43.857985
3502.101174	730155.541328	43.862989
3502.551240	730130.258951	43.867994
3502.374653	730097.948096	43.872999
3502.450837	730069.953714	43.878004
3502.706125	730036.085687	43.883009
3502.208674	730005.313105	43.888013
3502.461572	729971.148045	43.893018
3502.532054	729943.302745	43.898023
3502.230047	729912.596661	43.903028
3502.914878	729876.131339	43.908033
3502.296411	729854.986308	43.913037
3502.470845	729824.102333	43.918042
3502.495121	729795.075489	43.923047
3502.515542	729766.990197	43.928052
3502.714923	729724.759951	43.933057
3502.443979	729698.257788	43.938061
3502.728590	729663.392821	43.943066
3502.276985	729628.797597	43.948071
3502.416217	729590.835995	43.953076
3502.171112	729557.840883	43.958081
3502.041209	729538.397556	43.963085
3502.234068	729509.639088	43.968090
3502.322167	729482.532243	43.973095
3502.148888	729450.763090	43.978100
3502.492085	729433.916143	43.983105
3502.026824	729417.400490	43.988109
3502.321529	729380.303820	43.993114
3502.331284	729362.174363	43.998119
3502.003972	729325.724763	44.003124
3502.649382	729300.655277	44.008129
3502.293280	729277.781480	44.013133
3502.771158	729235.502808	44.018138
3502.448616	729214.356875	44.023143
3502.517179	729177.989976	44.028148
3502.631693	729152.660796	44.033153
3502.274402	729112.648937	44.038157
3502.279940	729083.275922	44.043162
3502.336168	729059.392470	44.048167
3502.507321	729033.805930	44.053172
3502.749165	728994.834004	44.058177
3502.254946	728972.229765	44.063181
3502.226839	728933.747818	44.068186
3502.432843	728902.706549	44.073191
3502.258429	728870.043727	44.078196
3502.335346	728843.877723	44.083201
3501.960532	728821.600121	44.088205
3502.520481	728792.778640	44.093210
3502.253473	728756.068883	44.098215
3502.364122	728737.574677	44.103220
3502.463318	728705.410982	44.108225
3502.133796	728684.066684	44.113229
3502.095703	728643.405515	44.118234
3502.387048	728629.686111	44.123239
3502.209122	728595.487202	44.128244
3502.286991	728580.614061	44.133249
3502.074734	728563.163358	44.138253
3502.253483	728530.639123	44.143258
3502.208561	728495.427181	44.148263
3502.119639	728478.550395	44.153268
3502.231903	728432.464057	44.158273
3502.205289	728416.864801	44.163277
3502.518156	728387.190961	44.168282
3502.400259	728360.659221	44.173287
3502.293253	728331.995546	44.178292
3502.820761	728300.403651	44.183297
3502.250254	728274.193888	44.188301
3502.445365	728234.185764	44.193306
3502.770109	728211.989373	44.198311
3502.472757	728173.250979	44.203316
3502.634303	728139.687742	44.208321
3502.335903	728114.621524	44.213325
3502.509382	728080.610242	44.218330
3502.476474	728053.320433	44.223335
3502.057145	728025.995128	44.228340
3502.624599	727980.574307	44.233345
3502.304559	727964.130845	44.238349
3502.381098	727931.026603	44.243354
3502.670782	727895.657863	44.248359
3502.674243	727877.922453	44.253364
3502.816950	727836.979781	44.258369
3502.555054	727800.363956	44.263373
3502.690958	727764.177816	44.268378
3502.989766	727739.804677	44.273383
3502.750947	727702.837834	44.278388
3502.684694	727652.268372	44.283393
3502.634033	727632.609278	44.288397
3502.545202	727595.022748	44.293402
3502.870631	727573.419000	44.298407
3502.848795	727531.312932	44.303412
3502.961047	727496.021241	44.308417
3502.729909	727468.316269	44.313421
3502.590708	727418.550042	44.318426
3502.454784	727371.656406	44.323431
3502.460700	727355.752511	44.328436
3502.378104	727314.596636	44.333441
3502.515181	727290.347892	44.338445
3501.906869	727261.663975	44.343450
3502.459793	727220.947883	44.348455
3502.110584	727196.778987	44.353460
3502.359790	727162.652324	44.358465
3502.206120	727145.585279	44.363469
3502.079676	727112.412082	44.368474
3502.407020	727097.049244	44.373479
3502.429982	727068.706526	44.378484
3502.634963	727039.541014	44.383489
3502.377107	727010.848014	44.388493
3502.352294	726976.518006	44.393498
3502.143207	726960.797402	44.398503
3501.950212	726917.428219	44.403508
3502.556793	726896.321353	44.408513
3502.297170	726871.938556	44.413517
3502.585469	726846.177231	44.418522
3502.352181	726815.200419	44.423527
3502.061137	726787.156192	44.428532
3502.178573	726756.418642	44.433537
3502.027514	726734.742558	44.438541
3502.216689	726705.033457	44.443546
3502.222569	726679.714511	44.448551
3502.533153	726655.782123	44.453556
3502.325264	726622.570814	44.458561
3502.349952	726601.410432	44.463565
3502.287440	726565.747154	44.468570
3502.294968	726530.419009	44.473575
3501.931379	726512.691572	44.478580
3502.154052	726479.904212	44.483585
3502.270910	726460.165151	44.488589
3502.304057	726439.250693	44.493594
3502.477173	726399.584059	44.498599
3502.208519	726381.047928	44.503604
3502.375338	726341.778435	44.508609
3502.034821	726315.871315	44.513613
3502.082960	726286.283033	44.518618
3502.008294	726270.340759	44.523623
3501.799269	726239.506416	44.528628
3502.399260	726223.155594	44.533633
3502.066028	726201.557665	44.538637
3502.264214	726168.971293	44.543642
3502.202808	726152.531113	44.548647
3502.223020	726127.703594	44.553652
3502.206363	726105.508205	44.558657
3501.754246	726083.780904	44.563661
3501.957716	726057.882434	44.568666
3502.145001	726031.689248	44.573671
3502.165866	726013.055029	44.578676
3502.111057	725976.496016	44.583681
3501.816152	725966.386833	44.588685
3502.227042	725919.791186	44.593690
3502.335629	725909.318145	44.598695
3501.820226	725886.163774	44.603700
3502.235189	725856.909909	44.608705
3502.110078	725840.330946	44.613709
3502.281428	725804.972684	44.618714
3502.243871	725781.788834	44.623719
3501.870064	725761.583873	44.628724
3501.855718	725734.580584	44.633729
3502.018595	725713.692453	44.638733
3501.959347	725695.615786	44.643738
3501.946726	725668.611996	44.648743
3502.121862	725648.415410	44.653748
3502.625440	725616.172946	44.658753
3502.362973	725597.733127	44.663757
3502.434273	725551.340005	44.668762
3502.274798	725522.823791	44.673767
3502.237603	725503.008707	44.678772
3502.342760	725474.547828	44.683777
3502.290263	725445.914614	44.688781
3502.290825	725424.408296	44.693786
3502.682570	725399.963342	44.698791
3502.226102	725360.990075	44.703796
3502.422307	725331.076629	44.708801
3502.668262	725312.651505	44.713805
3502.137539	725267.644391	44.718810
3502.329961	725246.403322	44.723815
3502.389879	725217.255240	44.728820
3502.495905	725182.251948	44.733825
3502.180028	725157.873317	44.738829
3502.444951	725126.708922	44.743834
3502.349108	725106.605212	44.748839
3502.220363	725074.960373	44.753844
3502.183052	725042.259671	44.758849
3502.177872	725027.492878	44.763853
3502.198457	724990.669272	44.768858
3502.245851	724977.231747	44.773863
3501.735199	724943.617517	44.778868
3502.527578	724914.645014	44.783873
3502.277504	724902.247516	44.788877
3502.256483	724864.785964	44.793882
3502.476811	724829.018979	44.798887
3502.023456	724814.722109	44.803892
3502.120354	724776.893824	44.808897
3502.305404	724765.514691	44.813901
3502.445576	724734.617157	44.818906
3502.363367	724700.386199	44.823911
3502.275565	724687.366942	44.828916
3502.102326	724638.233704	44.833921
3502.147649	724624.994179	44.838925
3502.072436	724597.798951	44.843930
3501.943543	724571.603656	44.848935
3501.977423	724558.068555	44.853940
3502.236334	724523.929334	44.858945
3502.209421	724516.945988	44.863949
3501.976591	724487.893118	44.868954
3502.287154	724466.927930	44.873959
3501.742230	724440.503410	44.878964
3501.885888	724417.384973	44.883969
3501.942300	724400.079355	44.888973
3501.787943	724377.852429	44.893978
3502.229102	724370.296234	44.898983
3502.069521	724327.899059	44.903988
3502.102070	724313.769053	44.908993
3502.286733	724279.789736	44.913997
3501.896503	724259.980266	44.919002
3502.427754	724229.561567	44.924007
3502.033251	724210.347413	44.929012
3502.248754	724174.380138	44.934017
3502.237178	724161.793541	44.939021
3502.381238	724124.350980	44.944026
3502.471278	724094.301852	44.949031
3502.240712	724068.022584	44.954036
3502.495963	724036.161793	44.959041
3502.714526	724010.254396	44.964045
3502.526082	723979.259490	44.969050
3502.502270	723957.455981	44.974055
3502.250921	723924.786108	44.979060
3502.434950	723886.542878	44.984065
3502.195621	723870.276138	44.989069
3502.313650	723834.719949	44.994074
3502.479210	723811.397952	44.999079
3502.332657	723779.304996	45.004084
3502.241023	723747.599376	45.009089
3502.361661	723721.806336	45.014093
3502.039774	723696.086132	45.019098
3502.105983	723669.161921	45.024103
3502.076667	723651.125393	45.029108
3502.404419	723616.524996	45.034113
3502.173480	723603.874562	45.039117
3502.012074	723572.080635	45.044122
3502.271707	723547.949355	45.049127
3502.218548	723520.647809	45.054132
3502.369868	723486.571590	45.059137
3502.314169	723464.425074	45.064141
3502.324455	723430.470993	45.069146
3502.195265	723398.522392	45.074151
3502.457592	723377.165860	45.079156
3502.285898	723346.264946	45.084161
3502.085827	723323.745311	45.089165
3502.174383	723296.270973	45.094170
3502.120399	723271.199230	45.099175
3502.121261	723247.605379	45.104180
3501.996253	723225.320941	45.109185
3501.931455	723198.020245	45.114189
3501.902033	723177.206941	45.119194
3502.193661	723150.640435	45.124199
3501.831038	723136.028284	45.129204
3502.022880	723109.131115	45.134209
3501.711123	723086.678803	45.139213
3501.854859	723064.746192	45.144218
3501.905098	723044.712515	45.149223
3501.886661	723024.888378	45.154228
3501.925349	723016.802452	45.159233
3501.788744	722987.926711	45.164237
3501.820349	722966.408862	45.169242
3502.161378	722955.447655	45.174247
3501.987835	722910.368790	45.179252
3502.031299	722891.128959	45.184257
3502.118227	722870.692263	45.189261
3502.009544	722858.615369	45.194266
3502.156860	722847.586799	45.199271
3501.792560	722827.026068	45.204276
3502.046011	722793.971122	45.209281
3502.166964	722768.026346	45.214285
3502.238684	722754.630763	45.219290
3502.327775	722712.630441	45.224295
3501.967591	722696.282156	45.229300
3502.187158	722661.993014	45.234305
3501.994680	722648.541651	45.239309
3502.026233	722611.755188	45.244314
3502.430758	722584.920413	45.249319
3501.995059	722569.674878	45.254324
3501.806605	722546.209360	45.259329
3502.088169	722508.439395	45.264333
3501.796588	722498.523674	45.269338
3502.098095	722475.274651	45.274343
3501.940627	722447.639746	45.279348
3502.229613	722435.199279	45.284353
3502.020370	722404.697603	45.289357
3501.710639	722387.993391	45.294362
3502.130853	722355.999803	45.299367
3501.861363	722335.471797	45.304372
3502.026483	722320.325092	45.309377
3502.048607	722302.723296	45.314381
3502.240683	722268.288337	45.319386
3502.490398	722247.426699	45.324391
3502.240455	722223.078085	45.329396
3502.208818	722187.985632	45.334401
3502.105593	722168.619572	45.339405
3502.400397	722137.240684	45.344410
3502.395532	722103.382798	45.349415
3501.794287	722087.519190	45.354420
3502.048013	722060.905863	45.359425
3501.843499	722026.832690	45.364429
3502.174494	722011.806813	45.369434
3502.366499	721997.398701	45.374439
3502.109887	721968.787046	45.379444
3502.398510	721939.589706	45.384449
3502.331796	721925.967720	45.389453
3502.028860	721893.744482	45.394458
3502.261370	721867.927231	45.399463
3501.797201	721837.366317	45.404468
3502.302369	721819.683904	45.409473
3502.183389	721790.553201	45.414477
3502.025834	721765.989717	45.419482
3502.276079	721724.404012	45.424487
3502.120829	721714.960645	45.429492
3502.258534	721676.367802	45.434497
3502.260834	721659.412398	45.439501
3502.056984	721623.354402	45.444506
3502.364701	721597.226458	45.449511
3502.069021	721581.113219	45.454516
3502.296918	721541.711660	45.459521
3502.151883	721528.548119	45.464525
3502.210452	721512.872148	45.469530
3502.203055	721473.707344	45.474535
3502.054002	721456.181534	45.479540
3502.124073	721411.649297	45.484545
3502.086887	721410.763085	45.489549
3501.812525	721386.515189	45.494554
3502.206011	721360.074899	45.499559
3501.958041	721342.862617	45.504564
3502.151702	721311.249382	45.509569
3502.149874	721284.873990	45.514573
3502.016099	721262.486551	45.519578
3502.241779	721249.955586	45.524583
3501.940193	721220.258022	45.529588
3502.098585	721201.590278	45.534593
3502.221921	721178.565300	45.539597
3501.954066	721162.744137	45.544602
3502.128167	721129.745214	45.549607
3501.861951	721109.808581	45.554612
3502.331107	721084.644017	45.559617
3502.043698	721062.529252	45.564621
3502.208355	721043.513062	45.569626
3502.257839	721018.417449	45.574631
3501.961338	720991.792198	45.579636
3502.054011	720956.773212	45.584641
3502.038015	720950.231278	45.589645
3502.205261	720914.555279	45.594650
3502.184300	720890.065854	45.599655
3502.019347	720864.955529	45.604660
3502.170830	720835.529002	45.609665
3501.914931	720814.003357	45.614669
3501.813227	720792.006016	45.619674
3502.199535	720780.687415	45.624679
3501.916123	720754.802970	45.629684
3501.864971	720736.218290	45.634689
3502.107082	720702.710648	45.639693
3502.035965	720682.046691	45.644698
3502.390848	720656.949247	45.649703
3502.131089	720639.638282	45.654708
3501.873949	720599.419692	45.659713
3502.229682	720578.585979	45.664717
3502.124404	720553.514462	45.669722
3502.315712	720533.302724	45.674727
3502.084679	720516.879264	45.679732
3502.200370	720482.251153	45.684737
3502.024653	720471.818073	45.689741
3502.155403	720439.517722	45.694746
3502.233657	720407.077145	45.699751
3502.302167	720388.422387	45.704756
3502.351004	720368.878316	45.709761
3502.097430	720334.360017	45.714765
3501.990194	720312.907746	45.719770
3502.196105	720280.693563	45.724775
3502.099542	720264.297031	45.729780
3501.976890	720239.425768	45.734785
3502.073798	720212.683610	45.739789
3501.878142	720191.642275	45.744794
3501.862887	720169.281945	45.749799
3501.843872	720154.905413	45.754804
3502.045003	720135.484456	45.759809
3502.281695	720115.412983	45.764813
3501.979883	720072.670341	45.769818
3502.341414	719976.760934	45.774823
3501.828064	719851.242362	45.779828
3501.448780	719654.193798	45.784833
3501.539915	719408.266886	45.789837
3501.388815	719114.318610	45.794842
3501.526034	718742.401115	45.799847
3501.162060	718326.557947	45.804852
3500.968637	717862.604763	45.809857
3500.609309	717339.478183	45.814861
3500.241637	716751.932619	45.819866
3499.997533	716094.723873	45.824871
3499.405746	715401.352881	45.829876
3498.785278	714630.624995	45.834881
3498.600367	713810.926187	45.839885
3497.726017	712933.445096	45.844890
3497.083204	712016.029086	45.849895
3496.494470	711024.195557	45.854900
3495.621721	709986.619786	45.859905
3495.084590	708887.890622	45.864909
3494.341766	707715.858146	45.869914
3493.807208	706499.627839	45.874919
3492.822673	705219.420880	45.879924
3492.195541	703885.211146	45.884929
3491.048465	702489.218505	45.889933
3489.730329	701050.092084	45.894938
3489.390447	699546.497339	45.899943
3488.060343	697984.841301	45.904948
3486.675869	696365.536507	45.909953
3485.904216	694704.854242	45.914957
3484.585196	692980.579888	45.919962
3483.354803	691204.016090	45.924967
3481.770466	689379.037930	45.929972
3480.576707	687491.558642	45.934977
3479.359642	685554.552846	45.939981
3477.752793	683578.408476	45.944986
3476.739189	681536.294601	45.949991
3474.818494	679462.192430	45.954996
3473.124129	677319.471978	45.960001
3471.607756	675148.715767	45.965005
3470.142152	672921.014414	45.970010
3468.434200	670644.356968	45.975015
3466.611800	668328.017027	45.980020
3464.647479	665967.932711	45.985025
3463.173720	663559.629791	45.990029
3460.958283	661121.247889	45.995034
3459.241200	658618.264935	46.000039
3457.271393	656093.207538	46.005044
3455.235920	653501.275561	46.010049
3453.225109	650897.867799	46.015053
3450.701023	648236.039435	46.020058
3448.993447	645547.774769	46.025063
3446.656601	642827.045960	46.030068
3444.614382	640053.322789	46.035073
3442.235026	637250.387742	46.040077
3439.935689	634410.547539	46.045082
3437.620041	631532.893289	46.050087
3435.406820	628633.654930	46.055092
3433.070583	625682.706319	46.060097
3430.727277	622700.834769	46.065101
3427.751118	619699.651638	46.070106
3425.275687	616649.385600	46.075111
3423.066079	613583.186876	46.080116
3420.061991	610485.174917	46.085121
3417.659252	607350.686381	46.090125
3414.760832	604194.734959	46.095130
3412.360129	601006.907255	46.100135
3409.378554	597790.677579	46.105140
3406.743225	594537.139263	46.110145
3403.965719	591266.899618	46.115149
3400.950940	587972.683264	46.120154
3398.245231	584639.058437	46.125159
3394.980121	581295.208797	46.130164
3392.042601	577935.759231	46.135169
3389.198443	574550.533302	46.140173
3386.202105	571137.397262	46.145178
3383.296866	567711.047715	46.150183
3380.100566	564256.191358	46.155188
3377.402331	560780.492698	46.160193
3374.154150	557278.124514	46.165197
3370.647794	553772.510586	46.170202
3367.845345	550224.741862	46.175207
3364.478015	546687.690834	46.180212
3361.093759	543119.784730	46.185217
3357.904702	539531.620146	46.190221
3354.479285	535932.649555	46.195226
3351.546815	532310.998302	46.200231
3347.584589	528673.121978	46.205236
3344.587300	525037.980095	46.210241
3341.230283	521379.746047	46.215245
3337.804579	517702.257703	46.220250
3334.283833	514017.089471	46.225255
3330.799512	510314.170062	46.230260
3327.286743	506614.843550	46.235265
3323.770695	502894.345923	46.240269
3320.404414	499178.999910	46.245274
3316.925378	495427.082410	46.250279
3312.976929	491688.377578	46.255284
3309.289870	487931.107150	46.260289
3305.752750	484172.197609	46.265293
3302.295360	480405.547212	46.270298
3298.506858	476627.789196	46.275303
3295.170859	472854.755855	46.280308
3291.211319	469058.373490	46.285313
3287.547030	465269.956191	46.290317
3283.685314	461455.040833	46.295322
3280.429786	457651.459489	46.300327
3276.298789	453843.304326	46.305332
3272.695073	450037.606699	46.310337
3268.932351	446215.831603	46.315341
3264.848489	442389.525921	46.320346
3261.167431	438572.533940	46.325351
3257.512545	434743.878593	46.330356
3253.940500	430924.569668	46.335361
3250.102239	427101.942930	46.340365
3246.208620	423274.554626	46.345370
3242.593532	419434.186871	46.350375
3238.339402	415598.163641	46.355380
3234.881781	411760.245793	46.360385
3230.918335	407925.715748	46.365389
3226.503870	404091.582584	46.370394
3222.708039	400252.958786	46.375399
3218.970747	396438.000427	46.380404
3214.859037	392606.117335	46.385409
3211.350535	388786.154663	46.390413
3206.915992	384958.912468	46.395418
3203.093921	381136.528546	46.400423
3199.213924	377325.357977	46.405428
3195.468641	373511.655999	46.410433
3191.596286	369700.437497	46.415437
3186.861591	365894.457727	46.420442
3183.325849	362089.220765	46.425447
3179.297420	358315.340528	46.430452
3175.241857	354516.795582	46.435457
3171.315928	350732.187385	46.440461
3167.109501	346961.982260	46.445466
3163.548062	343179.758861	46.450471
3159.568471	339415.705926	46.455476
3155.225704	335639.164827	46.460481
3151.397886	331873.543878	46.465485
3147.011476	328122.802581	46.470490
3143.223671	324365.231342	46.475495
3139.281662	320632.455396	46.480500
3135.456282	316895.807409	46.485505
3131.181661	313166.009226	46.490509
3127.307856	309447.542755	46.495514
3123.419953	305733.819806	46.500519
3119.192281	302044.716973	46.505524
3114.858925	298340.335464	46.510529
3111.223817	294656.254212	46.515533
3107.206465	290980.951848	46.520538
3103.143101	287299.208352	46.525543
3099.037272	283642.918615	46.530548
3094.942758	279981.527393	46.535553
3091.035028	276335.034715	46.540557
3086.738719	272696.137024	46.545562
3082.752019	269060.605495	46.550567
3078.747726	265441.469221	46.555572
3074.411418	261828.884883	46.560577
3070.590702	258222.622451	46.565581
3066.368295	254646.020780	46.570586
3062.520817	251055.055805	46.575591
3058.588801	247490.818163	46.580596
3054.302168	243924.507999	46.585601
3050.320389	240370.263928	46.590605
3046.212094	236841.639512	46.595610
3042.575694	233305.159146	46.600615
3038.448552	229777.087215	46.605620
3034.229263	226249.423049	46.610625
3030.340216	222752.028292	46.615629
3026.075300	219266.337002	46.620634
3022.228863	215767.274051	46.625639
3018.011369	212298.673762	46.630644
3014.135954	208834.366344	46.635649
3010.419522	205278.243756	46.640653
3006.071176	201845.938813	46.645658
3002.189957	198404.822478	46.650663
2997.799758	194984.073870	46.655668
2993.854934	191577.025951	46.660673
2990.110125	188169.434829	46.665677
2985.688763	184792.327462	46.670682
2981.925883	181406.854845	46.675687
2977.824718	178033.232909	46.680692
2973.502320	174672.632763	46.685697
2969.532097	171332.218289	46.690701
2965.527691	167994.807898	46.695706
2961.670193	164668.991994	46.700711
2958.043365	161355.742624	46.705716
2953.849315	158048.138694	46.710721
2949.719196	154759.373418	46.715725
2945.004808	151486.099012	46.720730
2940.980181	148219.336594	46.725735
2937.028660	144973.243872	46.730740
2933.064053	141736.218381	46.735745
2929.339813	138510.639478	46.740749
2924.876724	135298.771028	46.745754
2921.447682	132094.593031	46.750759
2916.931230	128910.749948	46.755764
2912.669425	125728.254555	46.760769
2908.560433	122562.784302	46.765773
2904.426201	119417.661478	46.770778
2900.717594	116278.738430	46.775783
2896.747856	113163.725391	46.780788
2892.365451	110059.731288	46.785793
2888.392491	106957.011623	46.790797
2884.052056	103873.705815	46.795802
2880.055333	100803.514489	46.800807
2875.741298	97763.825713	46.805812
2871.733122	94732.035616	46.810817
2867.603081	91708.631334	46.815821
2863.534469	88708.242578	46.820826
2859.544596	85722.008738	46.825831
2855.192756	82744.847018	46.830836
2851.233113	79784.024870	46.835841
2847.217819	76839.109070	46.840845
2842.700699	73923.938738	46.845850
2838.301443	71010.587682	46.850855
2834.084323	68136.259741	46.855860
2829.333197	65261.127832	46.860865
2825.467333	62419.406342	46.865869
2820.641468	59599.390976	46.870874
2816.268992	56805.970689	46.875879
2811.482035	54039.701246	46.880884
2806.674939	51296.496228	46.885889
2802.080617	48595.687749	46.890893
2796.846496	45920.827074	46.895898
2791.724090	43282.584870	46.900903
2784.921213	40710.893035	46.905908
2776.473387	38261.653959	46.910913
2767.300876	35906.123455	46.915917
2756.882716	33664.580803	46.920922
2745.320523	31572.115501	46.925927
2734.231244	29615.347233	46.930932
2723.404324	27814.265768	46.935937
2713.303610	26176.432907	46.940941
2703.138878	24699.211412	46.945946
2693.441304	23353.051348	46.950951
2684.570087	22151.115604	46.955956
2675.930256	21101.211748	46.960961
2668.498107	20159.520894	46.965965
2661.747462	19336.543931	46.970970
2655.454559	18602.850469	46.975975
2649.682603	17958.845192	46.980980
2644.140187	17391.459504	46.985985
2639.522774	16896.766921	46.990989
2635.163714	16471.557045	46.995994
2631.513516	16069.959661	47.000999
2627.970952	15717.515972	47.006004
2624.808768	15389.341422	47.011009
2621.642585	15089.371063	47.016013
2618.132248	14806.950688	47.021018
2615.437190	14522.956373	47.026023
2612.794135	14253.553912	47.031028
2609.859138	13999.124851	47.036033
2607.253403	13747.653852	47.041037
2604.456963	13501.275905	47.046042
2602.023936	13245.897205	47.051047
2599.008818	12986.513728	47.056052
2596.422583	12727.396970	47.061057
2593.880108	12467.540853	47.066061
2590.909626	12201.223390	47.071066
2588.359534	11926.445362	47.076071
2585.752549	11645.191282	47.081076
2582.662345	11359.939521	47.086081
2579.649319	11064.918404	47.091085
2576.940039	10764.342264	47.096090
2573.930543	10464.859147	47.101095
2570.380235	10160.602137	47.106100
2567.360535	9863.708380	47.111105
2564.611475	9548.894456	47.116109
2561.501222	9233.899874	47.121114
2558.168257	8896.244670	47.126119
2555.287372	8578.773547	47.131124
2551.660883	8251.134786	47.136129
2548.870081	7911.863685	47.141133
2545.127870	7584.957386	47.146138
2541.860371	7244.076473	47.151143
2538.378195	6904.797934	47.156148
2534.678280	6567.888179	47.161153
2531.366492	6228.943396	47.166157
2527.749027	5909.402722	47.171162
2524.311729	5558.484769	47.176167
2520.834373	5219.910266	47.181172
2517.264445	4903.480510	47.186177
2513.901448	4557.077981	47.191181
2510.609433	4236.280931	47.196186
2506.620141	3894.634253	47.201191
2502.934756	3567.639633	47.206196
2499.496805	3241.010089	47.211201
2495.819479	2921.567498	47.216205
2492.132913	2597.609992	47.221210
2488.342248	2276.429259	47.226215
2484.690989	1966.467613	47.231220
2480.857282	1666.032860	47.236225
2477.072255	1357.107214	47.241229
2472.831295	1077.810468	47.246234
2468.882384	788.848630	47.251239
2464.816498	518.969463	47.256244
2460.109079	271.446417	47.261249
2452.554750	131.635147	47.266253
2439.699304	163.320261	47.271258
2432.001492	164.895635	47.276263
2427.445173	167.013768	47.281268
2424.637787	172.430867	47.286273
2423.350440	167.182623	47.291277
2421.260182	168.565132	47.296282
2419.403169	169.531826	47.301287
2416.989940	162.981088	47.306292
2413.472719	166.932889	47.311297
2410.586851	162.809904	47.316301
2407.381934	163.219406	47.321306
2403.711942	159.286837	47.326311
2400.122312	159.303795	47.331316
2396.512552	163.038021	47.336321
2393.931856	163.038219	47.341325
2390.344842	166.662132	47.346330
2386.698763	161.090467	47.351335
2383.530929	158.159013	47.356340
2380.017363	161.566165	47.361345
2376.492972	166.577510	47.366349
2373.343755	170.595677	47.371354
2369.866422	164.168327	47.376359
2367.200832	158.619536	47.381364
2363.841387	161.263403	47.386369
2360.943035	162.229741	47.391373
2356.693737	153.133531	47.396378
2352.845555	159.422637	47.401383
2349.212446	147.931034	47.406388
2345.887275	161.064190	47.411393
2342.256414	142.566655	47.416397
2339.213198	163.245725	47.421402
2336.438256	157.276120	47.426407
2332.808946	159.534553	47.431412
2328.940682	161.697456	47.436417
2325.899606	145.702721	47.441421
2322.189885	161.716005	47.446426
2319.100187	154.152952	47.451431
2315.697796	154.365213	47.456436
2311.792903	155.494786	47.461441
2308.579354	152.511728	47.466445
2304.634338	159.134177	47.471450
2301.598596	152.815142	47.476455
2298.515181	153.083489	47.481460
2294.643001	165.485850	47.486465
2291.410618	156.602092	47.491469
2288.064626	165.113072	47.496474
2284.018755	160.665433	47.501479
2281.019079	156.778986	47.506484
2277.096121	159.423191	47.511489
2273.597071	155.262600	47.516493
2270.421935	159.810622	47.521498
2267.154924	158.709370	47.526503
2263.901792	160.458773	47.531508
2260.332343	151.745738	47.536513
2256.985378	154.559497	47.541517
2252.525207	156.438525	47.546522
2249.101511	161.389124	47.551527
2246.489658	154.862004	47.556532
2242.733215	156.975922	47.561537
2239.683013	158.311562	47.566541
2235.941241	155.798800	47.571546
2232.120494	152.667199	47.576551
2228.877520	157.019239	47.581556
2225.163072	154.331868	47.586561
2221.891249	145.782659	47.591565
2218.213167	145.404085	47.596570
2214.926474	150.588427	47.601575
2211.740897	157.214024	47.606580
2207.727465	154.372969	47.611585
2204.210185	140.604609	47.616589
2200.554875	146.052883	47.621594
2197.573033	140.996089	47.626599
2194.382460	141.441251	47.631604
2190.602827	147.112924	47.636609
2187.451794	141.257219	47.641613
2183.786782	142.366822	47.646618
2179.877037	141.709995	47.651623
2176.610842	140.517107	47.656628
2172.837392	139.588345	47.661633
2169.628086	134.036905	47.666637
2166.065586	141.022938	47.671642
2162.655086	150.861483	47.676647
2159.156123	140.190936	47.681652
2155.464230	142.192038	47.686657
2152.183948	147.502644	47.691661
2148.802959	147.867582	47.696666
2145.405506	147.673218	47.701671
2141.791065	136.085183	47.706676
2138.264868	146.330024	47.711681
2134.847291	137.617283	47.716685
2131.384067	143.093286	47.721690
2127.796747	146.824779	47.726695
2124.539996	141.154907	47.731700
2120.543000	144.718232	47.736705
2117.275274	137.514681	47.741709
2113.731917	144.625465	47.746714
2110.360354	139.770234	47.751719
2106.910493	139.353270	47.756724
2103.292069	138.654518	47.761729
2100.507977	147.978011	47.766733
2096.360999	141.263824	47.771738
2092.891869	148.728628	47.776743
2089.438070	139.448239	47.781748
2085.990770	144.189316	47.786753
2082.458876	143.280332	47.791757
2078.979830	137.665161	47.796762
2075.343995	147.031437	47.801767
2071.990865	142.869206	47.806772
2068.321464	136.812258	47.811777
2065.257695	137.843184	47.816781
2061.254010	138.962233	47.821786
2057.677717	143.473220	47.826791
2054.450651	140.925732	47.831796
2050.985549	152.361943	47.836801
2047.696649	140.258452	47.841805
2043.779726	143.453404	47.846810
2040.459005	131.221188	47.851815
2037.252705	138.683270	47.856820
2033.557615	145.029216	47.861825
2030.389430	145.312521	47.866829
2026.537533	143.519064	47.871834
2023.088637	134.181089	47.876839
2019.518980	137.913490	47.881844
2015.523737	139.939731	47.886849
2012.359305	144.095603	47.891853
2009.449710	134.637198	47.896858
2005.434005	137.853623	47.901863
2001.828991	139.449957	47.906868
1998.823758	133.494139	47.911873
1995.087943	132.808147	47.916877
1991.698753	140.496024	47.921882
1987.980675	138.830082	47.926887
1984.603860	126.913648	47.931892
1981.009966	138.132973	47.936897
1977.552679	128.776690	47.941901
1974.253441	137.709730	47.946906
1970.657596	139.119666	47.951911
1967.178113	133.410920	47.956916
1963.442097	141.895130	47.961921
1960.189733	135.833136	47.966925
1956.671809	138.476606	47.971930
1953.227040	131.950680	47.976935
1949.842487	132.278457	47.981940
1945.936928	134.134241	47.986945
1942.265649	128.206574	47.991949
1938.929363	127.541666	47.996954
1935.425935	129.291771	48.001959
1932.234148	125.089779	48.006964
1928.620006	136.076266	48.011969
1925.170640	124.202848	48.016973
1921.795109	129.894794	48.021978
1918.150317	134.764507	48.026983
1914.937292	139.588167	48.031988
1911.050407	140.679760	48.036993
1907.587865	131.420308	48.041997
1904.034035	130.116655	48.047002
1900.541459	142.294547	48.052007
1897.030789	134.255107	48.057012
1893.581888	140.684611	48.062017
1890.126224	128.215310	48.067021
1886.764187	135.279122	48.072026
1883.040482	134.972674	48.077031
1879.644948	131.894471	48.082036
1876.248042	124.912942	48.087041
1872.568412	128.937515	48.092045
1869.270057	133.357729	48.097050
1865.576237	132.446646	48.102055
1862.357177	122.286623	48.107060
1858.672876	135.857840	48.112065
1855.277830	125.385099	48.117069
1851.649257	128.553092	48.122074
1847.775774	129.539905	48.127079
1844.776888	126.089744	48.132084
1841.089297	136.630199	48.137089
1837.672588	125.591925	48.142093
1834.207722	121.418734	48.147098
1830.697081	124.616004	48.152103
1827.193646	123.702710	48.157108
1823.429991	138.476024	48.162113
1820.072961	125.059449	48.167117
1816.552196	135.171172	48.172122
1813.203661	135.890338	48.177127
1809.699769	125.312081	48.182132
1806.360857	132.629649	48.187137
1802.981988	124.620223	48.192141
1799.309111	120.841366	48.197146
1795.367132	127.552879	48.202151
1792.056470	126.939294	48.207156
1788.490389	130.429526	48.212161
1785.288685	130.398052	48.217165
1781.704171	122.477081	48.222170
1778.182982	123.739846	48.227175
1774.407357	130.890600	48.232180
1771.061480	135.415819	48.237185
1767.656159	122.258678	48.242189
1764.233522	126.827760	48.247194
1760.402374	126.193421	48.252199
1756.999026	120.020562	48.257204
1753.582573	132.550246	48.262209
1750.490633	128.317878	48.267213
1747.008875	130.310619	48.272218
1743.376711	129.220328	48.277223
1740.060171	117.399922	48.282228
1735.930943	127.924600	48.287233
1732.246064	122.959605	48.292237
1729.110530	121.279134	48.297242
1725.814882	133.165091	48.302247
1722.429725	130.769464	48.307252
1718.682946	133.349282	48.312257
1714.772509	124.235428	48.317261
1711.534632	128.691928	48.322266
1707.888217	127.410628	48.327271
1704.700687	118.374298	48.332276
1700.913578	129.264587	48.337281
1697.897905	119.052149	48.342285
1694.417875	131.357933	48.347290
1690.494448	124.482880	48.352295
1687.522472	126.271458	48.357300
1683.663132	120.833696	48.362305
1680.021004	128.197096	48.367309
1676.613048	127.545992	48.372314
1672.833204	125.990559	48.377319
1669.716128	122.287717	48.382324
1666.034689	126.922120	48.387329
1662.698316	113.506224	48.392333
1659.220566	127.164008	48.397338
1655.614670	119.689307	48.402343
1652.037812	118.553048	48.407348
1648.600541	124.114867	48.412353
1645.487834	126.197274	48.417357
1641.709163	123.256163	48.422362
1637.738530	125.590046	48.427367
1634.364020	120.622399	48.432372
1630.980709	125.979358	48.437377
1627.555387	114.401198	48.442381
1624.239220	121.036472	48.447386
1620.639004	123.081042	48.452391
1617.338839	119.893744	48.457396
1613.502700	125.363622	48.462401
1609.863015	120.360874	48.467405
1606.730724	117.760750	48.472410
1602.774166	121.371875	48.477415
1599.391573	119.878148	48.482420
1595.872750	125.772574	48.487425
1592.705351	124.202050	48.492429
1589.514747	112.157903	48.497434
1585.744007	119.039406	48.502439
1582.366854	117.805870	48.507444
1578.255964	120.114827	48.512449
1574.848047	119.387422	48.517453
1571.358214	124.804844	48.522458
1567.796460	115.870321	48.527463
1565.060278	113.907889	48.532468
1561.141609	115.012910	48.537473
1557.344492	121.758289	48.542477
1554.044825	121.917213	48.547482
1550.589730	116.216814	48.552487
1547.482509	114.541657	48.557492
1543.690424	120.787146	48.562497
1540.199481	113.680136	48.567501
1536.547162	114.773133	48.572506
1532.552715	126.803088	48.577511
1529.512351	118.439572	48.582516
1526.015419	114.252782	48.587521
1522.865022	107.547534	48.592525
1519.198919	120.020132	48.597530
1515.424032	117.907322	48.602535
1512.279278	114.294811	48.607540
1508.297468	115.925165	48.612545
1504.947253	107.208928	48.617549
1501.691294	112.114530	48.622554
1497.792046	114.356612	48.627559
1494.656288	104.468082	48.632564
1490.532969	119.272613	48.637569
1487.521036	107.097990	48.642573
1484.320713	110.052410	48.647578
1480.210152	112.811326	48.652583
1476.757983	115.288176	48.657588
1473.335831	122.341856	48.662593
1469.992656	116.711236	48.667597
1466.255586	117.430525	48.672602
1462.695455	124.923792	48.677607
1459.433849	112.465631	48.682612
1455.926781	118.839910	48.687617
1452.385060	117.477969	48.692621
1448.890942	116.563224	48.697626
1445.705984	122.770019	48.702631
1442.560941	110.839037	48.707636
1438.736600	117.965916	48.712641
1435.269396	119.812223	48.717645
1431.337962	111.444496	48.722650
1427.607263	127.082473	48.727655
1424.784641	118.612796	48.732660
1420.707983	116.519550	48.737665
1417.431302	117.301319	48.742669
1413.829446	112.384840	48.747674
1410.399803	113.541774	48.752679
1407.114800	112.477058	48.757684
1403.597170	119.639114	48.762689
1400.011429	117.021924	48.767693
1396.383594	110.718327	48.772698
1392.522619	112.412675	48.777703
1389.737325	118.610083	48.782708
1385.771738	108.287696	48.787713
1382.537133	107.002530	48.792717
1378.806010	111.400064	48.797722
1375.329239	107.743270	48.802727
1372.082243	108.364071	48.807732
1368.260235	109.950764	48.812737
1365.067732	107.679267	48.817741
1361.663077	111.840317	48.822746
1357.963848	113.016984	48.827751
1354.377971	108.842863	48.832756
1350.954355	107.575542	48.837761
1347.245654	109.670217	48.842765
1343.872833	116.349963	48.847770
1340.459084	113.641246	48.852775
1337.247810	108.754797	48.857780
1333.344369	113.270242	48.862785
1329.870942	113.205061	48.867789
1326.543240	109.340339	48.872794
1322.799133	104.496194	48.877799
1319.737948	105.668068	48.882804
1315.901169	109.824800	48.887809
1312.164607	107.489151	48.892813
1308.963238	110.904445	48.897818
1305.124076	113.303898	48.902823
1301.784625	109.340494	48.907828
1298.173093	101.946568	48.912833
1294.704687	108.506375	48.917837
1291.324719	107.305295	48.922842
1287.956269	116.518559	48.927847
1284.724922	104.995861	48.932852
1280.750371	106.699603	48.937857
1277.045933	110.566506	48.942861
1274.018736	109.314227	48.947866
1270.551475	115.248306	48.952871
1267.013446	112.369957	48.957876
1263.227417	110.150864	48.962881
1259.994194	114.944726	48.967885
1256.376935	108.249959	48.972890
1252.583432	114.074190	48.977895
1249.293713	105.452358	48.982900
1245.496130	110.524625	48.987905
1242.076329	112.417110	48.992909
1239.329474	109.528961	48.997914
1235.639389	107.752840	49.002919
1232.464774	108.347763	49.007924
1228.191141	110.490732	49.012929
1224.436360	111.898496	49.017933
1221.255578	105.401561	49.022938
1217.541026	115.191674	49.027943
1214.453819	101.710713	49.032948
1210.804341	108.701107	49.037953
1207.208603	111.215700	49.042957
1203.905274	107.747440	49.047962
1200.145408	115.056243	49.052967
1196.846277	112.102541	49.057972
1192.947337	109.197089	49.062977
1189.689985	110.879825	49.067981
1186.739580	106.050611	49.072986
1182.592964	109.100698	49.077991
1179.278082	106.289526	49.082996
1176.103797	108.947196	49.088001
1172.154456	113.915355	49.093005
1168.889366	99.903602	49.098010
1164.844876	97.252337	49.103015
1161.675458	96.543829	49.108020
1158.289414	99.751568	49.113025
1154.398867	104.951756	49.118029
1151.429907	98.315664	49.123034
1147.938067	103.585903	49.128039
1144.542763	99.823867	49.133044
1140.431620	109.244474	49.138049
1137.440109	107.691961	49.143053
1133.810372	110.719191	49.148058
1130.226338	101.952333	49.153063
1126.748243	103.272200	49.158068
1123.190932	107.629154	49.163073
1119.315223	98.422914	49.168077
1116.301728	100.885513	49.173082
1112.921866	105.117625	49.178087
1109.433920	94.935785	49.183092
1105.641451	102.551970	49.188097
1101.790817	104.982887	49.193101
1098.648947	101.061963	49.198106
1095.208916	104.097125	49.203111
1091.727738	100.189289	49.208116
1088.164294	96.727424	49.213121
1084.705536	104.084796	49.218125
1081.606882	100.988514	49.223130
1077.599210	108.428365	49.228135
1074.092181	99.430770	49.233140
1070.724208	107.685429	49.238145
1067.260464	100.922229	49.243149
1063.819545	101.882368	49.248154
1060.132100	114.552383	49.253159
1056.665284	103.670689	49.258164
1052.916572	114.618027	49.263169
1049.336690	108.224710	49.268173
1046.261245	108.438488	49.273178
1042.654840	104.815435	49.278183
1039.406605	98.134631	49.283188
1035.627538	109.729328	49.288193
1032.113669	112.112906	49.293197
1028.658793	104.066174	49.298202
1025.003139	103.509799	49.303207
1021.579086	109.331725	49.308212
1018.064047	101.853415	49.313217
1014.983068	115.855642	49.318221
1011.247631	109.549057	49.323226
1007.453359	115.593637	49.328231
1004.335890	106.968188	49.333236
1000.845845	106.660323	49.338241
997.076517	102.732922	49.343245
993.558780	97.830914	49.348250
990.117278	96.697663	49.353255
986.447619	102.574632	49.358260
982.742334	103.886790	49.363265
979.266646	113.969493	49.368269
976.437784	102.714192	49.373274
972.483815	107.669268	49.378279
969.217388	96.677952	49.383284
965.741139	102.067500	49.388289
961.912401	108.220230	49.393293
958.611756	98.593242	49.398298
955.180071	101.613509	49.403303
951.863409	95.958598	49.408308
947.798262	100.361777	49.413313
944.201608	100.268924	49.418317
941.036660	100.923625	49.423322
937.456838	100.599675	49.428327
934.338606	90.904459	49.433332
930.620657	99.564792	49.438337
926.926576	101.096751	49.443341
923.821482	87.682938	49.448346
919.842258	98.146727	49.453351
916.619815	98.057721	49.458356
913.198864	100.026217	49.463361
909.316364	101.970803	49.468365
906.288182	91.690020	49.473370
902.308283	100.079537	49.478375
898.737465	93.408587	49.483380
895.879507	99.684187	49.488385
892.142346	97.718016	49.493389
888.334220	92.083661	49.498394
884.929106	104.376950	49.503399
881.628019	97.684688	49.508404
878.198323	102.206412	49.513409
874.944409	97.632256	49.518413
871.078959	95.256340	49.523418
867.078451	96.404888	49.528423
863.753561	97.859851	49.533428
860.772054	97.706370	49.538433
856.714750	100.630282	49.543437
853.372085	99.443495	49.548442
849.539649	98.832636	49.553447
846.259281	102.061799	49.558452
843.159919	94.969949	49.563457
839.505639	107.060574	49.568461
836.291393	99.347570	49.573466
832.650589	99.746767	49.578471
829.227185	100.193284	49.583476
825.394977	94.895480	49.588481
821.808023	103.800040	49.593485
818.533591	91.272932	49.598490
815.012816	106.726987	49.603495
811.358720	98.069687	49.608500
807.770969	97.216912	49.613505
804.456825	87.299843	49.618509
801.040479	89.283250	49.623514
797.323784	91.310618	49.628519
793.842770	99.016419	49.633524
790.365244	93.195451	49.638529
786.925896	95.290420	49.643533
783.508941	100.481243	49.648538
779.762690	95.519534	49.653543
776.350518	96.563148	49.658548
773.171519	97.074066	49.663553
769.506018	91.449380	49.668557
765.867417	83.545364	49.673562
762.146809	96.321500	49.678567
759.044813	94.188611	49.683572
755.636297	88.377177	49.688577
751.805080	102.313209	49.693581
748.633313	88.046045	49.698586
744.604773	94.165294	49.703591
741.405846	82.891285	49.708596
738.026779	87.708036	49.713601
734.683189	80.113610	49.718605
731.149778	85.482192	49.723610
727.429308	95.151081	49.728615
723.006429	92.262874	49.733620
720.314191	87.985073	49.738625
716.977980	96.040924	49.743629
713.318628	75.662067	49.748634
709.714972	82.371733	49.753639
706.169136	92.407602	49.758644
702.722926	77.558559	49.763649
699.267261	94.628344	49.768653
695.803907	85.424754	49.773658
692.079529	93.328951	49.778663
689.027246	92.041563	49.783668
685.734904	101.274984	49.788673
681.835005	100.618402	49.793677
678.558230	100.267813	49.798682
674.790878	99.721722	49.803687
671.301370	96.872542	49.808692
667.918760	97.716578	49.813697
664.076960	98.187054	49.818701
660.926650	93.771754	49.823706
657.156418	100.733001	49.828711
653.860049	89.386381	49.833716
649.943295	88.880224	49.838721
646.665894	100.651499	49.843725
643.095760	93.779378	49.848730
640.068831	92.266025	49.853735
636.455516	89.593649	49.858740
633.017645	88.259587	49.863745
629.134400	91.742962	49.868749
625.921984	82.787805	49.873754
622.008176	90.637752	49.878759
618.719181	89.816217	49.883764
615.252194	93.355253	49.888769
611.505072	92.937888	49.893773
608.105587	85.828195	49.898778
604.704912	87.678324	49.903783
601.229056	88.400296	49.908788
597.938737	89.538537	49.913793
594.505638	94.154367	49.918797
591.225766	84.146169	49.923802
586.963887	92.211603	49.928807
583.542473	84.100334	49.933812
580.130059	89.231546	49.938817
576.387946	99.846407	49.943821
573.178851	87.015467	49.948826
569.605906	95.508021	49.953831
566.033571	91.963213	49.958836
562.912484	88.446161	49.963841
559.472529	86.541218	49.968845
556.167851	81.454161	49.973850
552.148693	85.694572	49.978855
548.644352	89.005601	49.983860
545.458739	85.301116	49.988865
541.504654	90.229336	49.993869
538.000692	80.468428	49.998874
534.772200	86.563019	50.003879
531.163640	89.940839	50.008884
527.376879	95.103446	50.013889
524.011964	90.526428	50.018893
520.691506	84.887893	50.023898
517.112723	86.068401	50.028903
513.451764	76.913070	50.033908
510.552079	90.540412	50.038913
506.541324	89.258625	50.043917
503.268956	77.294660	50.048922
499.736093	83.327356	50.053927
496.636622	76.593769	50.058932
492.996147	79.207884	50.063937
488.871262	88.485262	50.068941
485.478355	81.781690	50.073946
481.970409	84.903531	50.078951
478.415425	86.169920	50.083956
475.075275	85.412412	50.088961
471.158521	85.243860	50.093965
468.240473	85.460212	50.098970
464.618520	84.949838	50.103975
461.213287	83.382592	50.108980
457.670320	81.669025	50.113985
454.132311	92.099235	50.118989
450.616968	85.921921	50.123994
446.993946	89.193074	50.128999
444.011617	80.718787	50.134004
440.098148	90.576512	50.139009
436.380659	77.585928	50.144013
433.228234	84.241059	50.149018
429.459208	85.159291	50.154023
425.741296	85.973359	50.159028
422.754092	81.598347	50.164033
418.946812	91.164812	50.169037
415.675712	84.602757	50.174042
412.093975	78.329512	50.179047
408.733132	89.083661	50.184052
405.418588	81.363346	50.189057
401.370845	92.247957	50.194061
398.092450	84.910808	50.199066
394.488703	86.753068	50.204071
390.863599	85.512349	50.209076
387.632131	87.779827	50.214081
383.764378	91.324785	50.219085
380.307461	83.039206	50.224090
376.777122	83.604808	50.229095
373.212272	82.279145	50.234100
370.259320	77.353861	50.239105
366.580790	86.730333	50.244109
363.445152	74.683085	50.249114
359.709977	84.272586	50.254119
356.219379	84.514116	50.259124
352.278871	91.115231	50.264129
348.873603	89.598795	50.269133
345.783698	78.723460	50.274138
342.186446	88.875839	50.279143
338.625250	83.579617	50.284148
335.018251	93.995283	50.289153
331.608169	87.481362	50.294157
328.172786	75.696286	50.299162
324.436236	81.961542	50.304167
320.767189	84.055616	50.309172
317.494240	83.123715	50.314177
313.876429	82.414857	50.319181
310.431733	81.115338	50.324186
306.851006	82.396388	50.329191
303.404066	80.067949	50.334196
299.965431	80.148186	50.339201
296.315183	82.404338	50.344205
293.045631	73.189167	50.349210
289.562736	86.219525	50.354215
285.925739	85.540506	50.359220
282.440874	74.724092	50.364225
279.098377	78.795312	50.369229
275.477395	78.195151	50.374234
271.525924	83.721290	50.379239
268.275125	86.021655	50.384244
264.791478	81.587250	50.389249
261.027079	85.882837	50.394253
257.969819	76.118298	50.399258
254.766255	87.580007	50.404263
251.087065	87.452251	50.409268
247.541609	86.938476	50.414273
243.668783	77.340132	50.419277
240.634765	74.436637	50.424282
236.879383	82.997320	50.429287
233.122826	81.779484	50.434292
229.763039	75.899852	50.439297
226.706082	75.644644	50.444301
223.272711	80.160152	50.449306
219.266234	83.168179	50.454311
215.639676	81.732491	50.459316
212.307387	78.549436	50.464321
208.722504	89.231484	50.469325
205.679231	75.852858	50.474330
202.087715	79.034927	50.479335
198.146970	73.593084	50.484340
194.973569	75.922721	50.489345
191.158109	89.996060	50.494349
187.831694	75.756585	50.499354
184.137303	77.646188	50.504359
180.933988	84.581246	50.509364
177.381339	74.773085	50.514369
173.836691	83.027200	50.519373
170.370915	76.823579	50.524378
166.800782	74.485457	50.529383
163.242605	92.374309	50.534388
160.034635	75.285079	50.539393
156.224634	82.907071	50.544397
152.938067	80.180823	50.549402
149.512935	78.135825	50.554407
146.018201	78.012748	50.559412
142.319020	76.214607	50.564417
138.573812	81.422748	50.569421
135.383080	83.860872	50.574426
131.991647	76.548389	50.579431
128.314023	81.730353	50.584436
125.094858	75.564679	50.589441
121.107173	85.091583	50.594445
117.834003	82.761957	50.599450
113.757301	82.063139	50.604455
110.353123	82.882565	50.609460
107.289427	82.803791	50.614465
103.518112	75.807608	50.619469
100.682419	76.150681	50.624474
96.913546	75.109253	50.629479
93.169788	78.193678	50.634484
89.765371	75.201451	50.639489
86.116397	86.958619	50.644493
82.756724	79.858777	50.649498
79.283977	79.032367	50.654503
75.645423	82.055382	50.659508
71.991430	72.618711	50.664513
68.570651	81.633641	50.669517
65.281361	77.602943	50.674522
61.711278	75.489865	50.679527
58.257263	81.781766	50.684532
55.120257	73.033652	50.689537
51.300639	75.600436	50.694541
47.613658	72.023563	50.699546
44.388290	76.294998	50.704551
40.417302	71.375335	50.709556
37.202726	75.167242	50.714561
33.561668	79.832526	50.719565
29.991878	79.883392	50.724570
26.677346	84.225649	50.729575
22.888828	77.079852	50.734580
20.252069	70.194845	50.739585
16.386061	66.887013	50.744589
12.875063	77.490263	50.749594
9.160136	79.167927	50.754599
5.557817	70.474608	50.759604
2.059747	73.656165	50.764609