Tue Jun 21 10:58:48 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.154668	102.519121	0.000000
1.335631	122.099501	0.005005
1.729608	123.146088	0.010010
1.427416	122.233973	0.015014
1.412558	102.024110	0.020019
1.326507	97.332576	0.025024
0.960761	98.767424	0.030029
0.881961	103.860889	0.035034
0.531973	94.842505	0.040038
0.693180	74.374022	0.045043
0.876709	76.963284	0.050048
0.487642	59.730856	0.055053
0.142607	45.126151	0.060058
-0.485068	36.641791	0.065062
-0.557537	24.155533	0.070067
-0.886386	22.417066	0.075072
-1.444993	9.628300	0.080077
-1.481092	4.666266	0.085082
-2.113875	12.877345	0.090086
-2.533454	0.984149	0.095091
-2.642977	2.141535	0.100096
-2.924215	-4.304100	0.105101
-3.158056	-12.902786	0.110106
-3.987406	3.962311	0.115110
-3.749302	-1.053219	0.120115
-3.890279	-5.599268	0.125120
-4.196641	-0.816841	0.130125
-3.858860	-2.839548	0.135130
-5.003306	7.665204	0.140134
-4.778955	-6.550473	0.145139
-5.178884	1.641378	0.150144
-5.160698	6.139183	0.155149
-5.350008	-2.502403	0.160154
-6.461958	5.112551	0.165158
-6.574229	-3.303019	0.170163
-6.792804	4.918397	0.175168
-7.012587	1.229784	0.180173
-6.927270	-2.041477	0.185178
-6.983923	9.123777	0.190182
-7.193734	-1.684881	0.195187
-8.113493	3.289703	0.200192
-8.354873	7.721564	0.205197
-8.268171	-1.164444	0.210202
-8.493203	9.493329	0.215206
-8.271266	-5.224556	0.220211
-8.916049	3.951292	0.225216
-9.559427	6.210390	0.230221
-9.507363	3.153414	0.235226
-10.066458	6.484280	0.240230
-9.932455	-4.414265	0.245235
-9.987494	-8.793590	0.250240
-10.285435	8.809152	0.255245
-10.973303	5.311322	0.260250
-11.598385	12.133283	0.265254
-11.479604	-0.946432	0.270259
-11.573076	1.143457	0.275264
-11.378608	2.157163	0.280269
-11.400607	-1.797844	0.285274
-12.517246	6.272149	0.290278
-12.855842	-12.295025	0.295283
-12.864441	-4.279475	0.300288
-13.277438	2.012844	0.305293
-13.180790	-3.733861	0.310298
-13.270196	3.060758	0.315302
-13.452099	1.422082	0.320307
-14.138915	-3.648267	0.325312
-14.516266	-4.069986	0.330317
-14.511047	-0.695623	0.335322
-15.082339	-3.781779	0.340326
-15.163138	-1.719248	0.345331
-14.959798	3.738110	0.350336
-15.441648	-1.624886	0.355341
-16.001905	-4.810549	0.360346
-16.094600	-4.214600	0.365350
-16.208742	-5.309990	0.370355
-16.425953	-1.374874	0.375360
-16.447977	-8.484833	0.380365
-17.468094	-7.300971	0.385370
-17.633277	-3.910624	0.390374
-17.876843	-1.577235	0.395379
-17.924526	-1.442605	0.400384
-18.022410	-3.525577	0.405389
-17.818046	-8.572221	0.410394
-18.403315	-4.202010	0.415398
-19.328024	-5.695376	0.420403
-19.437781	-6.083857	0.425408
-19.568422	0.888282	0.430413
-19.544957	-13.159539	0.435418
-19.742679	-1.042877	0.440422
-19.691374	-9.026140	0.445427
-19.448378	-0.717774	0.450432
-20.446684	-0.601542	0.455437
-21.099136	-6.894334	0.460442
-21.146765	2.745812	0.465446
-21.102086	-4.783082	0.470451
-21.178117	-2.273395	0.475456
-22.677736	-4.281706	0.480461
-22.370073	-10.249043	0.485466
-23.030902	-2.560008	0.490470
-22.562141	-2.442626	0.495475
-22.766083	-4.858891	0.500480
-23.089832	-7.230057	0.505485
-22.763583	-6.852473	0.510490
-23.197253	-4.665202	0.515494
-23.731352	1.119899	0.520499
-24.233125	-1.814772	0.525504
-24.268679	-5.358067	0.530509
-24.709029	-5.183669	0.535514
-24.694314	-1.182176	0.540518
-24.827890	-6.692039	0.545523
-25.528540	-5.108793	0.550528
-25.670127	-2.314155	0.555533
-26.031694	-13.831747	0.560538
-26.027487	-2.214627	0.565542
-25.942477	-5.355596	0.570547
-26.344879	-4.204369	0.575552
-27.138279	-0.744717	0.580557
-27.235845	-7.135516	0.585562
-27.451266	-7.807826	0.590566
-27.572866	-6.538329	0.595571
-27.702078	-10.348890	0.600576
-27.761316	0.267803	0.605581
-28.433801	-16.204041	0.610586
-29.049215	-3.804499	0.615590
-29.067818	-13.539350	0.620595
-29.118821	-11.244759	0.625600
-29.336377	3.463012	0.630605
-29.456491	-12.213694	0.635610
-29.525942	-4.332120	0.640614
-29.799894	-2.260493	0.645619
-30.389414	-3.527968	0.650624
-30.701943	2.683580	0.655629
-30.765683	-13.422977	0.660634
-30.700233	1.887347	0.665638
-31.288338	-5.993184	0.670643
-32.017133	-2.620006	0.675648
-32.186358	6.914380	0.680653
-32.347960	-0.849910	0.685658
-32.472792	5.320886	0.690662
-32.499752	5.693620	0.695667
-32.344728	6.050819	0.700672
-33.103896	-9.086715	0.705677
-33.590332	-1.990142	0.710682
-33.782954	-0.452547	0.715686
-33.936673	-3.865372	0.720691
-33.599442	4.121720	0.725696
-34.226079	-3.187467	0.730701
-34.257583	-5.833765	0.735706
-35.058529	3.044912	0.740710
-35.328316	-12.361523	0.745715
-35.427965	0.705038	0.750720
-35.924452	-6.990766	0.755725
-35.401857	-1.275483	0.760730
-35.597619	3.104620	0.765734
-36.282428	7.910455	0.770739
-36.846964	3.964784	0.775744
-37.030348	3.331766	0.780749
-37.199364	-0.860162	0.785754
-37.109934	1.113794	0.790758
-37.586469	-2.940182	0.795763
-38.281468	-2.810042	0.800768
-38.686945	-1.108536	0.805773
-38.647241	0.171940	0.810778
-38.803577	4.883348	0.815782
-38.757902	-4.159845	0.820787
-38.906274	-6.402582	0.825792
-39.137578	0.400734	0.830797
-39.032144	-7.499141	0.835802
-40.112127	6.006830	0.840806
-40.335914	5.896727	0.845811
-40.122557	-0.355732	0.850816
-40.596577	3.294146	0.855821
-40.308080	-2.434799	0.860826
-41.401864	4.519245	0.865830
-41.746505	0.312594	0.870835
-41.843430	-3.202185	0.875840
-41.994826	-0.540108	0.880845
-41.710798	-1.418661	0.885850
-42.038078	4.491833	0.890854
-42.411626	-0.000899	0.895859
-43.021764	-0.950409	0.900864
-43.683028	-1.425944	0.905869
-43.702209	-1.976044	0.910874
-43.559995	9.149760	0.915878
-43.590010	-2.139178	0.920883
-43.452856	1.637403	0.925888
-44.488740	0.442076	0.930893
-44.867272	-10.547208	0.935898
-45.324195	1.720123	0.940902
-45.425309	1.679885	0.945907
-45.287896	-2.924303	0.950912
-45.606831	-4.856607	0.955917
-45.509780	-8.365424	0.960922
-46.211998	0.194392	0.965926
-46.552730	-1.611956	0.970931
-46.806204	-2.412149	0.975936
-47.072448	-0.155910	0.980941
-46.683348	-12.017843	0.985946
-47.015344	-2.143340	0.990950
-47.781158	-8.387555	0.995955
-48.207638	-5.176921	1.000960
-48.473186	1.140313	1.005965
-48.316389	-10.795037	1.010970
-48.568739	-0.836636	1.015974
-48.663714	0.685775	1.020979
-48.710505	4.274767	1.025984
-49.752050	1.163487	1.030989
-49.936842	-12.648759	1.035994
-50.369682	2.122683	1.040998
-50.520080	-5.021071	1.046003
-50.013393	-4.021778	1.051008
-50.264307	5.043064	1.056013
-50.329679	-0.591166	1.061018
-51.071902	1.528216	1.066022
-51.700574	-2.598439	1.071027
-51.570266	1.637877	1.076032
-51.983009	4.493604	1.081037
-51.877263	1.221723	1.086042
-52.185523	1.983218	1.091046
-52.638907	-3.221685	1.096051
-53.008858	0.927575	1.101056
-53.144359	4.757994	1.106061
-53.214993	10.293086	1.111066
-53.412882	8.025199	1.116070
-54.104397	4.891865	1.121075
-54.646621	1.411957	1.126080
-55.006762	3.800964	1.131085
-54.585344	-2.748403	1.136090
-54.999648	2.163790	1.141094
-55.010171	-1.598151	1.146099
-54.999015	-6.903074	1.151104
-55.689871	5.905215	1.156109
-55.962197	-2.087993	1.161114
-56.425495	2.951306	1.166118
-56.604149	-4.176717	1.171123
-56.425605	-1.475155	1.176128
-56.886443	-0.160328	1.181133
-56.668641	0.237779	1.186138
-57.676870	10.611449	1.191142
-58.193513	-0.625312	1.196147
-58.098956	1.230578	1.201152
-58.456761	7.759242	1.206157
-58.142190	-7.815009	1.211162
-58.439300	6.096675	1.216166
-58.485961	2.144964	1.221171
-58.789496	1.516059	1.226176
-60.067175	2.023309	1.231181
-59.650489	-1.848258	1.236186
-59.991909	-0.655821	1.241190
-59.886018	7.345901	1.246195
-59.746576	3.801053	1.251200
-60.942334	7.332282	1.256205
-61.111203	1.996786	1.261210
-61.415659	4.685989	1.266214
-61.496607	1.576056	1.271219
-61.751060	1.653368	1.276224
-61.731902	6.904426	1.281229
-61.826888	-4.961997	1.286234
-62.575756	-7.070946	1.291238
-62.859606	-0.781466	1.296243
-63.361798	0.290387	1.301248
-63.366117	8.848685	1.306253
-63.173909	0.738880	1.311258
-63.308184	6.237940	1.316262
-63.688487	-2.322477	1.321267
-64.312706	-4.499232	1.326272
-64.870332	-5.036920	1.331277
-64.715518	-2.170404	1.336282
-64.801391	4.739857	1.341286
-65.034914	-4.207368	1.346291
-65.021635	-1.548883	1.351296
-65.696069	-2.382366	1.356301
-66.079639	-2.788053	1.361306
-66.373759	6.294008	1.366310
-66.152072	-2.088064	1.371315
-66.394440	-10.726770	1.376320
-67.334409	2.357204	1.381325
-67.813871	-10.866730	1.386330
-67.886695	-2.324324	1.391334
-67.634727	-3.244533	1.396339
-67.806080	-7.361675	1.401344
-68.024187	3.462281	1.406349
-67.853265	-8.499878	1.411354
-68.296227	-1.642369	1.416358
-68.889706	-1.817340	1.421363
-69.019689	-6.327909	1.426368
-69.347044	-0.545473	1.431373
-69.533302	-11.782476	1.436378
-70.380084	-2.834837	1.441382
-70.808886	-8.157669	1.446387
-70.884479	-5.318904	1.451392
-71.172652	5.305708	1.456397
-71.023531	-8.764696	1.461402
-71.025488	-4.423203	1.466406
-71.088576	-2.325126	1.471411
-70.891624	-2.624690	1.476416
-71.738232	2.875718	1.481421
-72.131789	-0.904876	1.486426
-72.563566	6.910611	1.491430
-72.777243	-7.495361	1.496435
-72.478324	-8.974694	1.501440
-73.613564	-5.011660	1.506445
-73.884668	-0.437533	1.511450
-74.243555	4.585265	1.516454
-74.495617	-5.637012	1.521459
-74.046544	-1.139534	1.526464
-74.607874	7.816484	1.531469
-74.499653	-1.143137	1.536474
-74.527272	-5.192126	1.541478
-74.878995	7.185855	1.546483
-75.073597	-0.982628	1.551488
-75.676688	-2.209172	1.556493
-75.755679	-10.188808	1.561498
-75.904897	7.743900	1.566502
-76.669145	-0.034241	1.571507
-76.890205	-2.606126	1.576512
-77.332360	5.621137	1.581517
-77.313214	-6.041988	1.586522
-77.352339	2.232977	1.591526
-77.457441	0.278878	1.596531
-77.365300	2.265013	1.601536
-78.559581	-1.043358	1.606541
-78.534748	-1.200555	1.611546
-79.217526	4.941088	1.616550
-78.828562	-3.311610	1.621555
-78.986638	-6.127568	1.626560
-78.956969	8.107494	1.631565
-79.484072	-7.302102	1.636570
-80.161147	-8.517378	1.641574
-80.308358	-12.143408	1.646579
-80.382941	-2.844534	1.651584
-80.456149	3.732504	1.656589
-80.721551	1.279455	1.661594
-81.718875	-1.141569	1.666598
-81.798478	-11.382930	1.671603
-81.784734	9.731814	1.676608
-81.948139	5.411876	1.681613
-81.907203	-2.535727	1.686618
-82.267499	7.522054	1.691622
-82.694899	0.759841	1.696627
-83.153958	1.084752	1.701632
-83.799267	-1.287617	1.706637
-83.496528	2.913628	1.711642
-83.895087	-3.466982	1.716646
-83.996794	5.092642	1.721651
-83.873841	-1.284950	1.726656
-84.624685	-0.252820	1.731661
-84.794473	1.589229	1.736666
-85.425256	6.281337	1.741670
-85.368538	-2.263246	1.746675
-85.642292	2.839778	1.751680
-85.875379	11.163053	1.756685
-85.367785	-3.109199	1.761690
-85.881609	3.871345	1.766694
-86.394521	1.807779	1.771699
-86.637016	-2.122546	1.776704
-87.252152	2.826660	1.781709
-87.005782	9.066020	1.786714
-87.374861	5.300118	1.791718
-87.862854	10.520125	1.796723
-88.116164	3.816695	1.801728
-88.336756	5.668934	1.806733
-88.451053	1.367505	1.811738
-88.248261	1.451969	1.816742
-88.881122	0.688959	1.821747
-89.258325	-8.965975	1.826752
-89.888239	-2.052047	1.831757
-89.936774	-7.621374	1.836762
-90.339332	4.217820	1.841766
-90.147427	-2.841332	1.846771
-90.260205	-2.414722	1.851776
-90.295658	-8.642741	1.856781
-90.963599	-1.593262	1.861786
-91.711072	2.043696	1.866790
-91.931077	8.762658	1.871795
-91.647863	-2.506914	1.876800
-91.798892	6.054367	1.881805
-91.963483	-1.563592	1.886810
-92.535816	0.519371	1.891814
-93.118186	-0.391120	1.896819
-93.013676	-6.937333	1.901824
-93.274784	-0.536180	1.906829
-93.240106	-15.294862	1.911834
-93.471719	-1.204398	1.916838
-93.622501	-5.789861	1.921843
-94.090403	-15.655518	1.926848
-94.560849	-5.694941	1.931853
-94.559955	-5.671956	1.936858
-94.490447	-3.579855	1.941862
-95.873006	-7.909017	1.946867
-96.034551	-7.999629	1.951872
-96.299038	-10.523865	1.956877
-96.479824	-0.623100	1.961882
-96.384297	-5.380386	1.966886
-96.749592	-15.485626	1.971891
-96.622613	-11.049460	1.976896
-96.629171	-3.249939	1.981901
-96.626619	-10.850978	1.986906
-97.307610	-9.860015	1.991910
-97.740971	-10.406636	1.996915
-97.722676	-6.842400	2.006912
-97.719380	-8.122220	2.016909
-97.496673	-4.164035	2.026906
-96.973330	-5.470908	2.036902
-96.313294	2.283173	2.046899
-95.316556	-4.459434	2.056896
-94.973847	-6.438015	2.066893
-95.047780	-8.704431	2.076890
-94.188513	-7.327814	2.086886
-93.636069	-8.901899	2.096883
-93.769927	-3.195305	2.106880
-92.781238	-8.273304	2.116877
-92.407520	-15.015466	2.126874
-91.723052	-5.880164	2.136870
-91.213023	-9.372495	2.146867
-90.821567	-10.047775	2.156864
-89.967143	-1.940203	2.166861
-89.720450	-2.649005	2.176858
-89.468699	-3.345801	2.186854
-88.167718	-7.623928	2.196851
-88.026574	-6.703150	2.206848
-87.753808	-2.140938	2.216845
-87.606118	-2.823267	2.226842
-86.483296	-3.530959	2.236838
-86.516598	4.590272	2.246835
-85.706178	-1.505010	2.256832
-84.802143	-5.207032	2.266829
-85.254291	-2.706103	2.276826
-84.607907	-1.061075	2.286822
-83.827525	5.110179	2.296819
-82.975492	-1.334214	2.306816
-82.502192	-5.742594	2.316813
-82.294899	-5.900324	2.326810
-81.698967	-7.747758	2.336806
-80.959445	-4.567703	2.346803
-80.615838	-5.943796	2.356800
-80.599843	-10.155317	2.366797
-79.585031	-8.964305	2.376794
-79.220703	-8.151818	2.386790
-78.855670	-2.651339	2.396787
-77.863726	-6.131606	2.406784
-77.722770	-6.831392	2.416781
-77.668584	-14.858682	2.426778
-76.602063	1.397951	2.436774
-76.455486	-3.340227	2.446771
-75.211904	-0.771598	2.456768
-74.861568	-6.569977	2.466765
-74.621942	-6.451701	2.476762
-74.667247	-4.774708	2.486758
-73.928418	1.741102	2.496755
-73.275141	-4.113970	2.506752
-72.236991	-1.756521	2.516749
-71.783586	-5.717828	2.526746
-71.239263	-0.314220	2.536742
-71.304486	-1.399531	2.546739
-71.100358	-0.580863	2.556736
-69.999822	-8.293017	2.566733
-69.743931	-12.020074	2.576730
-69.357933	-6.588665	2.586726
-68.696129	-0.710550	2.596723
-68.302711	-6.199334	2.606720
-67.277049	-2.464820	2.616717
-66.775455	3.416121	2.626714
-66.957380	0.362427	2.636710
-66.175017	-2.100932	2.646707
-65.198891	-3.571702	2.656704
-65.034691	-3.331866	2.666701
-64.891267	-7.115381	2.676698
-64.414918	-3.911693	2.686694
-63.398200	1.895594	2.696691
-63.265703	2.516685	2.706688
-62.665165	-1.730395	2.716685
-61.591214	-4.901189	2.726682
-61.639812	-2.717633	2.736678
-61.679626	-5.207243	2.746675
-60.754579	-4.088691	2.756672
-60.161138	8.509767	2.766669
-59.570069	1.994193	2.776666
-58.911431	0.254533	2.786662
-58.732372	-6.337831	2.796659
-58.447810	-0.065096	2.806656
-57.724749	-9.212036	2.816653
-57.270550	-6.641695	2.826650
-56.342702	-5.892696	2.836646
-56.153089	-6.083063	2.846643
-56.013387	-5.815065	2.856640
-54.807899	-8.631635	2.866637
-54.391276	-4.450873	2.876634
-54.494520	-3.274648	2.886630
-53.261372	-5.123678	2.896627
-52.592336	-5.308876	2.906624
-52.683438	-5.898506	2.916621
-52.732731	-3.625527	2.926618
-51.498575	-9.541625	2.936614
-51.241672	-7.402737	2.946611
-50.751318	-7.447892	2.956608
-49.641015	-7.689769	2.966605
-49.412244	-11.860853	2.976602
-49.566725	-4.388184	2.986598
-48.635606	-4.693053	2.996595
-47.962806	-6.075056	3.006592
-47.901357	-3.663732	3.016589
-47.053688	-11.219996	3.026586
-46.507124	-0.133802	3.036582
-46.120704	-2.937624	3.046579
-45.148012	-8.946358	3.056576
-44.926970	-6.197314	3.066573
-44.822870	-10.509575	3.076570
-44.419220	-1.989070	3.086566
-43.520521	-5.270134	3.096563
-43.564938	-0.791525	3.106560
-42.351077	-8.804001	3.116557
-41.613644	-7.314330	3.126554
-41.718547	-2.996418	3.136550
-41.260693	-3.340077	3.146547
-40.350893	-1.983474	3.156544
-40.110992	-4.766389	3.166541
-39.936378	-3.315498	3.176538
-38.623240	-2.085558	3.186534
-38.865630	-3.139356	3.196531
-38.056884	-4.435595	3.206528
-37.348886	-5.983667	3.216525
-36.992891	-4.243318	3.226522
-36.849082	-9.214187	3.236518
-36.129442	-6.961062	3.246515
-35.385816	-6.178191	3.256512
-35.164289	-9.261356	3.266509
-34.189049	-13.277070	3.276506
-33.691697	-5.618341	3.286502
-33.677267	-8.093224	3.296499
-33.671622	-6.532945	3.306496
-32.596208	-7.805177	3.316493
-32.134444	-10.835656	3.326490
-31.322533	-9.840624	3.336486
-30.869290	-7.953964	3.346483
-30.641764	-6.042767	3.356480
-30.199806	-6.249039	3.366477
-29.300567	-5.434835	3.376474
-28.993096	-6.284896	3.386470
-28.820260	-6.921793	3.396467
-28.003529	-9.365545	3.406464
-27.316545	-8.762381	3.416461
-27.359321	-13.173216	3.426458
-26.561528	-11.547326	3.436454
-26.095527	-7.856254	3.446451
-25.807257	-3.279413	3.456448
-24.728517	-10.154533	3.466445
-24.382901	-5.445125	3.476442
-24.257840	-6.628536	3.486438
-23.692418	-7.365221	3.496435
-23.147479	1.180497	3.506432
-22.163993	-7.547811	3.516429
-21.651312	-3.864864	3.526426
-21.121981	-3.331618	3.536422
-21.150437	-0.970409	3.546419
-20.852763	-2.311032	3.556416
-20.168710	-4.259990	3.566413
-19.557655	-1.496298	3.576410
-19.146038	-0.475873	3.586406
-18.382970	-2.482767	3.596403
-18.240567	-4.341235	3.606400
-17.525581	-5.793842	3.616397
-16.616738	-5.992271	3.626394
-16.446396	-8.589791	3.636390
-16.592133	-2.571808	3.646387
-15.521385	-8.126325	3.656384
-15.193464	-7.930395	3.666381
-13.963761	-8.605779	3.676378
-14.017005	-8.360360	3.686374
-13.530128	-3.935354	3.696371
-13.289544	-4.178024	3.706368
-12.355476	-11.528087	3.716365
-11.992633	-5.367697	3.726362
-11.823254	-12.256613	3.736358
-10.739332	-1.254261	3.746355
-10.458811	-4.411806	3.756352
-10.248759	-10.217380	3.766349
-9.341834	-14.169415	3.776346
-8.776293	-8.613219	3.786342
-8.549622	-10.160811	3.796339
-8.428699	-6.976698	3.806336
-7.447133	-16.185407	3.816333
-7.190785	-5.105285	3.826330
-5.883607	-7.897585	3.836326
-5.788840	-6.352854	3.846323
-5.705899	-5.447133	3.856320
-5.359960	-7.886617	3.866317
-4.264449	-7.980609	3.876314
-4.244409	-11.273240	3.886310
-3.733049	-0.387288	3.896307
-3.218157	11.228562	3.906304
-2.537779	13.355618	3.916301
-2.013337	18.506665	3.926298
-2.063180	31.190148	3.936294
-1.245900	49.546392	3.946291
-1.169908	64.183939	3.956288
-0.717262	84.376515	3.966285
-0.067581	105.193267	3.976282
0.000000	125.149273	3.981286
0.428368	131.601473	3.986291
0.537423	147.650848	3.991296
0.897865	149.653355	3.996301
0.902874	158.140340	4.001306
0.871797	156.114561	4.006310
1.255649	159.078160	4.011315
0.874660	174.662095	4.016320
1.052015	172.226861	4.021325
1.159620	182.165438	4.026330
1.330935	192.715473	4.031334
1.455951	189.056741	4.036339
1.237398	196.589948	4.041344
1.636009	200.840304	4.046349
1.268102	184.457907	4.051354
1.166323	196.246849	4.056358
1.482314	193.703404	4.061363
1.276125	193.688261	4.066368
1.687755	185.242071	4.071373
1.639014	185.694193	4.076378
1.412978	192.421733	4.081382
1.432662	184.426042	4.086387
1.239941	190.207170	4.091392
1.533878	185.609171	4.096397
1.272336	180.306123	4.101402
1.292102	196.472357	4.106406
1.301862	192.967688	4.111411
1.388183	188.819065	4.116416
1.852259	198.054914	4.121421
1.334676	195.313051	4.126426
1.461405	201.200335	4.131430
1.655947	189.660548	4.136435
1.400133	196.450841	4.141440
1.524024	192.896882	4.146445
1.252663	187.452981	4.151450
1.220873	192.579341	4.156454
1.529729	192.538897	4.161459
1.235900	203.880320	4.166464
1.766526	214.859077	4.171469
1.909725	217.841227	4.176474
1.952521	212.533354	4.181478
1.641061	202.656234	4.186483
1.790379	204.037371	4.191488
1.543232	188.426880	4.196493
1.489201	198.810980	4.201498
1.629552	218.890955	4.206502
2.101383	224.365698	4.211507
1.775968	209.429221	4.216512
2.009227	198.984346	4.221517
1.630647	198.772985	4.226522
1.486265	196.822007	4.231526
1.998989	209.360504	4.236531
1.716645	228.225636	4.241536
1.793260	226.320543	4.246541
1.556738	230.402182	4.251546
1.828128	229.290291	4.256550
1.826024	224.907264	4.261555
1.983366	224.995512	4.266560
2.238179	225.353360	4.271565
1.673146	221.006130	4.276570
1.648979	234.394482	4.281574
2.052083	216.179982	4.286579
1.895899	227.635580	4.291584
2.100518	219.044077	4.296589
2.026382	218.987924	4.301594
1.701095	224.626637	4.306598
1.905697	215.741503	4.311603
2.316393	223.732730	4.316608
2.329769	221.778515	4.321613
2.360964	228.616607	4.326618
2.236337	229.965361	4.331622
2.319472	217.224269	4.336627
2.054204	210.536334	4.341632
1.823722	216.010158	4.346637
1.859437	227.823321	4.351642
2.103031	226.965071	4.356646
2.225725	219.794731	4.361651
2.018436	223.361808	4.366656
2.297939	222.100770	4.371661
2.091559	226.846976	4.376666
2.025841	229.692831	4.381670
2.126339	221.641115	4.386675
1.816270	224.674251	4.391680
2.148783	228.415186	4.396685
2.149886	226.523387	4.401690
2.200645	230.561399	4.406694
2.305047	230.972572	4.411699
2.327127	232.448586	4.416704
2.469377	222.808505	4.421709
2.465066	225.924802	4.426714
2.012424	233.432263	4.431718
2.377441	219.561117	4.436723
2.313624	224.640892	4.441728
2.302933	222.402947	4.446733
2.550180	224.640093	4.451738
2.360218	231.352402	4.456742
2.386489	224.240257	4.461747
2.579908	233.896675	4.466752
2.401530	226.253051	4.471757
2.765029	229.383231	4.476762
2.463227	225.320972	4.481766
2.646996	217.645206	4.486771
2.849992	221.099743	4.491776
2.667421	223.004120	4.496781
2.411234	221.090203	4.501786
2.559908	219.613040	4.506790
2.645110	216.840815	4.511795
2.454114	225.439230	4.516800
2.383093	226.095535	4.521805
2.691314	230.854010	4.526810
2.497478	234.168048	4.531814
2.933525	214.615288	4.536819
2.699463	221.359365	4.541824
2.487670	216.730650	4.546829
2.666076	224.208989	4.551834
2.681834	224.399419	4.556838
2.923285	214.326142	4.561843
2.420704	203.869324	4.566848
2.454944	208.330588	4.571853
2.644430	214.679117	4.576858
2.552589	223.871668	4.581862
2.752841	221.258979	4.586867
2.251141	232.474412	4.591872
2.740563	220.246600	4.596877
2.785150	225.009460	4.601882
2.503836	222.818698	4.606886
2.706918	221.670166	4.611891
2.525516	231.069757	4.616896
2.732267	227.238231	4.621901
2.791495	219.722407	4.626906
2.552278	224.689936	4.631910
2.644460	224.764307	4.636915
2.727262	226.268548	4.641920
2.693982	221.508840	4.646925
2.551822	229.291079	4.651930
2.808515	241.500812	4.656934
3.354855	244.015813	4.661939
3.138037	235.815747	4.666944
3.008710	221.276585	4.671949
2.617287	225.822156	4.676954
2.775253	232.954599	4.681958
2.868444	227.984306	4.686963
2.878117	246.661192	4.691968
2.989392	253.916227	4.696973
3.115021	254.441892	4.701978
3.098529	257.159818	4.706982
2.944816	245.696802	4.711987
3.062887	247.128702	4.716992
3.029140	248.509572	4.721997
3.291270	238.422593	4.727002
3.191642	234.488076	4.732006
3.120704	227.347232	4.737011
2.833148	230.140628	4.742016
3.054092	228.131911	4.747021
3.170373	247.295732	4.752026
3.068759	242.216795	4.757030
3.523950	234.882458	4.762035
3.111504	235.808031	4.767040
3.170994	225.339028	4.772045
3.238433	224.876402	4.777050
3.335087	222.009729	4.782054
3.460462	227.073765	4.787059
3.174169	234.982490	4.792064
3.266315	221.691309	4.797069
3.101806	223.710110	4.802074
3.019484	229.663597	4.807078
3.147680	223.744045	4.812083
3.056017	235.542985	4.817088
3.195370	236.046446	4.822093
3.454746	247.389435	4.827098
3.492540	252.857326	4.832102
3.125914	239.001351	4.837107
2.978516	258.873282	4.842112
3.186671	253.873878	4.847117
3.086690	261.979293	4.852122
3.159690	254.048541	4.857126
3.256207	251.389878	4.862131
3.375148	263.966594	4.867136
3.663426	257.082778	4.872141
3.660574	257.348911	4.877146
3.256668	259.714020	4.882150
3.545484	256.808021	4.887155
3.309171	262.486675	4.892160
3.644117	264.462240	4.897165
3.583290	260.856763	4.902170
3.316639	262.011968	4.907174
3.601971	261.509312	4.912179
3.422040	267.401818	4.917184
3.413464	264.196569	4.922189
3.520909	262.236638	4.927194
3.321779	265.902029	4.932198
3.560530	253.530008	4.937203
3.466273	257.756225	4.942208
3.583879	255.099989	4.947213
3.491039	257.496467	4.952218
3.280200	262.926207	4.957222
3.657341	244.430231	4.962227
3.578655	257.017369	4.967232
3.525358	269.804161	4.972237
3.662075	273.981872	4.977242
3.735734	288.700499	4.982246
4.285801	283.974807	4.987251
3.818585	271.376905	4.992256
3.363686	258.012493	4.997261
3.858736	258.991636	5.002266
3.577188	257.793311	5.007270
3.758407	258.135524	5.012275
3.959662	261.674226	5.017280
3.868753	264.341131	5.022285
3.795044	259.482531	5.027290
3.434313	261.618685	5.032294
3.671374	281.527226	5.037299
4.077634	280.268675	5.042304
3.863219	286.959206	5.047309
3.711719	285.884188	5.052314
3.930930	289.059587	5.057318
3.928965	290.538009	5.062323
3.805090	292.662769	5.067328
3.797566	285.946524	5.072333
3.772802	288.735091	5.077338
3.639004	294.071767	5.082342
3.622680	289.504593	5.087347
3.835876	293.485727	5.092352
4.083135	281.965559	5.097357
3.901530	282.724836	5.102362
3.763773	280.638561	5.107366
4.089235	290.913901	5.112371
3.974048	297.771133	5.117376
3.876638	289.516731	5.122381
3.691536	288.224879	5.127386
3.772362	294.641163	5.132390
4.396422	301.153384	5.137395
3.877011	288.067612	5.142400
3.813574	300.240221	5.147405
4.145441	304.326028	5.152410
3.998059	324.812547	5.157414
3.839559	320.601619	5.162419
3.848582	321.410042	5.167424
4.019469	322.706907	5.172429
4.217193	322.010368	5.177434
3.804448	322.106785	5.182438
4.361309	328.818208	5.187443
3.915188	327.715803	5.192448
4.342271	314.081361	5.197453
4.158807	319.574076	5.202458
4.200727	333.809196	5.207462
4.452223	323.539414	5.212467
4.501805	328.083421	5.217472
4.197889	322.426411	5.222477
4.504478	326.148179	5.227482
4.332916	321.914746	5.232486
4.175631	323.532559	5.237491
4.361486	322.924419	5.242496
4.233144	321.591196	5.247501
4.145235	320.351722	5.252506
4.176572	330.170217	5.257510
4.102264	316.952104	5.262515
4.210141	326.161568	5.267520
4.280127	333.344148	5.272525
4.544942	333.891563	5.277530
4.464156	350.299771	5.282534
4.479414	343.258266	5.287539
4.449042	345.594684	5.292544
4.718246	350.998044	5.297549
4.650877	332.376854	5.302554
4.573659	331.236054	5.307558
4.529148	321.123629	5.312563
4.271830	332.422593	5.317568
4.294487	331.425688	5.322573
4.566082	347.904599	5.327578
4.727094	351.383088	5.332582
4.911686	349.174356	5.337587
4.282956	339.065126	5.342592
4.935860	332.557011	5.347597
4.772896	336.065861	5.352602
3.884551	334.249312	5.357606
4.356222	344.450351	5.362611
4.732104	358.862458	5.367616
4.852236	353.978636	5.372621
4.971214	357.553284	5.377626
5.021065	356.897018	5.382630
4.831391	344.634747	5.387635
4.808081	330.519172	5.392640
4.580843	340.020746	5.397645
5.000854	324.003040	5.402650
4.622555	331.983094	5.407654
4.761899	321.636176	5.412659
4.516007	324.250611	5.417664
4.694095	349.789758	5.422669
5.096194	348.448418	5.427674
5.008974	361.822260	5.432678
5.061828	330.731536	5.437683
4.555615	319.056684	5.442688
4.536721	324.774345	5.447693
4.869442	346.422836	5.452698
4.808330	349.639142	5.457702
5.187427	357.264678	5.462707
5.068351	361.065627	5.467712
4.722651	342.660818	5.472717
4.851098	342.754049	5.477722
4.527095	350.913973	5.482726
4.803063	344.789933	5.487731
5.236174	355.259233	5.492736
5.009073	358.799232	5.497741
5.042146	349.372515	5.502746
5.091919	358.100843	5.507750
4.855998	355.193905	5.512755
4.474251	362.646668	5.517760
4.779460	361.749199	5.522765
4.804470	357.186803	5.527770
4.573917	363.402877	5.532774
4.902337	359.933216	5.537779
4.514627	362.998378	5.542784
4.893053	376.113572	5.547789
5.109539	376.389562	5.552794
4.913194	378.709266	5.557798
5.173171	379.877520	5.562803
5.044850	382.346988	5.567808
4.823047	382.655498	5.572813
4.881597	371.694589	5.577818
5.092557	381.940603	5.582822
5.082393	377.946636	5.587827
5.372546	380.050009	5.592832
5.033174	387.846634	5.597837
4.908954	389.855627	5.602842
4.996972	382.498944	5.607846
5.042832	390.445691	5.612851
5.100744	409.531760	5.617856
5.184105	402.841461	5.622861
5.435412	417.147560	5.627866
5.330983	418.247299	5.632870
5.466103	414.621968	5.637875
5.171864	414.112666	5.642880
5.407669	410.683787	5.647885
5.563578	417.421586	5.652890
5.200614	415.905596	5.657894
5.394349	402.081398	5.662899
5.552112	414.957485	5.667904
5.219394	413.951738	5.672909
5.575032	405.673558	5.677914
5.234062	415.891406	5.682918
5.469518	410.114457	5.687923
5.815907	410.737367	5.692928
5.647723	411.929558	5.697933
5.390300	412.839731	5.702938
5.468311	419.367043	5.707942
5.444611	419.905011	5.712947
5.685202	414.016899	5.717952
5.480613	413.486436	5.722957
5.750278	415.317329	5.727962
5.608802	417.266035	5.732966
5.368180	417.325661	5.737971
5.233685	417.645762	5.742976
5.058715	411.864158	5.747981
5.585962	409.444947	5.752986
5.364871	419.538554	5.757990
5.379105	409.254525	5.762995
5.403556	415.767025	5.768000
5.356132	425.725313	5.773005
5.721247	420.344853	5.778010
5.504641	439.299998	5.783014
5.581630	436.191447	5.788019
5.675784	443.186748	5.793024
5.647123	448.044689	5.798029
6.026677	444.434917	5.803034
5.839426	447.033741	5.808038
5.989835	444.530701	5.813043
6.007909	441.851053	5.818048
5.445638	429.465312	5.823053
5.671107	439.139442	5.828058
5.955335	442.232866	5.833062
6.011009	442.660995	5.838067
5.918275	445.854338	5.843072
6.023439	438.085904	5.848077
5.820385	426.920814	5.853082
5.824301	424.601288	5.858086
6.125294	416.992249	5.863091
5.994723	425.426055	5.868096
5.614431	423.321116	5.873101
5.716035	419.028015	5.878106
5.640847	443.251966	5.883110
5.836233	437.790675	5.888115
6.053533	445.464952	5.893120
6.060735	453.184879	5.898125
6.086611	452.424832	5.903130
5.790882	457.366864	5.908134
6.129860	448.448491	5.913139
5.983153	455.766470	5.918144
6.007302	442.923070	5.923149
6.337874	454.410910	5.928154
6.006142	447.754401	5.933158
6.248372	449.611548	5.938163
5.905024	458.317216	5.943168
5.776353	457.480737	5.948173
5.948172	460.884644	5.953178
6.110030	459.569856	5.958182
6.117865	455.145847	5.963187
6.241525	457.700686	5.968192
6.176854	451.608938	5.973197
6.415042	454.797213	5.978202
6.154392	457.717621	5.983206
6.242670	451.567391	5.988211
6.395531	451.740055	5.993216
5.801763	448.088399	5.998221
6.007123	446.369166	6.003226
5.967195	459.350845	6.008230
6.027188	452.275439	6.013235
6.093627	452.370848	6.018240
6.005744	455.564771	6.023245
5.927040	455.076215	6.028250
6.032021	460.047601	6.033254
6.185368	444.143985	6.038259
6.290144	446.551182	6.043264
6.302770	453.722004	6.048269
6.434194	447.390184	6.053274
5.788321	450.783268	6.058278
6.215844	446.075848	6.063283
6.020194	445.422935	6.068288
6.187321	458.812167	6.073293
6.315493	458.364342	6.078298
6.274111	446.706351	6.083302
6.081734	444.608378	6.088307
6.354599	442.869283	6.093312
6.285592	444.625822	6.098317
6.154282	439.798805	6.103322
6.040876	444.273931	6.108326
6.000510	451.208432	6.113331
6.207765	457.803949	6.118336
6.439803	462.959528	6.123341
6.468829	461.581683	6.128346
6.088754	459.146359	6.133350
6.234502	453.798464	6.138355
6.181998	456.113699	6.143360
6.154812	450.109085	6.148365
6.364949	444.667846	6.153370
6.257065	459.631007	6.158374
6.564877	451.919389	6.163379
6.124278	455.544100	6.168384
5.911391	455.762134	6.173389
6.482722	451.743291	6.178394
6.308842	453.895890	6.183398
6.464811	450.318406	6.188403
6.293792	459.639848	6.193408
6.312474	451.884150	6.198413
6.319035	451.627753	6.203418
5.963425	448.873820	6.208422
6.049208	449.379254	6.213427
6.007562	448.984611	6.218432
6.295604	455.567539	6.223437
6.466022	450.230558	6.228442
6.263097	454.207430	6.233446
6.329182	449.406332	6.238451
6.265376	454.786135	6.243456
6.427928	449.544390	6.248461
6.564904	448.220699	6.253466
6.348951	459.154932	6.258470
6.307671	456.927939	6.263475
6.128128	452.959633	6.268480
6.038434	448.991053	6.273485
6.022304	439.655706	6.278490
6.027748	452.916994	6.283494
6.043022	450.004948	6.288499
6.086558	448.691600	6.293504
6.317783	455.397801	6.298509
6.536525	446.506444	6.303514
6.264072	452.292189	6.308518
6.440099	447.083734	6.313523
6.183363	453.022775	6.318528
6.129389	451.495279	6.323533
6.448542	453.122024	6.328538
6.071059	447.717706	6.333542
5.929636	443.514572	6.338547
6.072812	445.578751	6.343552
6.172631	452.937997	6.348557
6.307265	447.813359	6.353562
6.001939	453.554819	6.358566
6.206377	456.109897	6.363571
5.843554	443.832608	6.368576
5.683120	452.774982	6.373581
6.116295	448.451435	6.378586
6.013274	452.211661	6.383590
6.131856	449.357892	6.388595
5.868605	456.220768	6.393600
6.043637	455.395764	6.398605
6.264658	447.845341	6.403610
5.786725	457.547162	6.408614
5.814183	449.276931	6.413619
6.072189	471.009603	6.418624
6.066108	480.322097	6.423629
6.347682	480.406548	6.428634
6.022760	490.274470	6.433638
6.818109	482.375539	6.438643
6.259723	472.728186	6.443648
5.839450	467.926713	6.448653
6.611403	470.868336	6.453658
6.295106	461.595313	6.458662
6.054966	450.697426	6.463667
5.806909	452.435268	6.468672
6.076149	468.331363	6.473677
6.412124	472.592167	6.478682
6.101529	480.244356	6.483686
6.118419	482.874306	6.488691
6.299906	486.968094	6.493696
6.213394	488.085000	6.498701
6.486252	471.656771	6.503706
6.476397	477.100269	6.508710
6.259562	457.416145	6.513715
6.115376	448.770188	6.518720
6.120319	453.522910	6.523725
6.421987	449.366776	6.528730
5.847005	464.545824	6.533734
5.865853	453.663658	6.538739
6.378030	473.442623	6.543744
6.144618	475.997591	6.548749
6.242257	461.735768	6.553754
6.098668	468.802024	6.558758
6.612344	472.889937	6.563763
6.348539	461.098267	6.568768
6.059234	460.460468	6.573773
6.399365	450.754718	6.578778
6.193953	453.707617	6.583782
6.146462	448.428033	6.588787
6.210842	449.725971	6.593792
6.029043	455.567747	6.598797
6.238739	451.753636	6.603802
6.148910	447.350539	6.608806
6.134397	457.934290	6.613811
6.295829	453.748492	6.618816
5.825444	459.683841	6.623821
6.078865	451.933474	6.628826
6.025045	477.335210	6.633830
6.328443	483.977966	6.638835
6.292486	487.747421	6.643840
6.048457	484.338980	6.648845
6.404546	476.659613	6.653850
6.163731	473.493765	6.658854
5.986100	461.197240	6.663859
6.207473	472.606678	6.668864
6.432467	484.280552	6.673869
6.319064	458.712604	6.678874
5.931776	466.887410	6.683878
6.242067	478.106496	6.688883
6.383075	480.259841	6.693888
6.069048	468.507662	6.698893
6.341702	463.892385	6.703898
5.803250	473.256132	6.708902
6.450861	466.466644	6.713907
6.491359	464.962576	6.718912
6.028310	455.308129	6.723917
6.045015	452.146410	6.728922
5.941827	460.952618	6.733926
6.194628	476.511627	6.738931
6.479112	478.898937	6.743936
6.245704	476.016227	6.748941
6.325781	463.117569	6.753946
6.066399	466.034216	6.758950
6.246116	458.751115	6.763955
6.216349	455.696352	6.768960
6.227612	454.389532	6.773965
6.642832	452.026163	6.778970
5.783137	455.996549	6.783974
5.846380	460.295606	6.788979
6.245616	477.036501	6.793984
6.181501	481.925386	6.798989
6.486546	484.157144	6.803994
6.129689	471.148887	6.808998
5.973734	458.606048	6.814003
6.288595	468.332884	6.819008
5.938541	472.180792	6.824013
6.409962	480.212814	6.829018
6.342162	483.015251	6.834022
6.270816	463.709598	6.839027
6.282494	455.381196	6.844032
6.077399	461.049425	6.849037
6.480588	457.740624	6.854042
6.137110	458.334705	6.859046
6.209383	455.980766	6.864051
6.425050	448.233890	6.869056
6.016225	451.330587	6.874061
6.313090	447.421331	6.879066
6.043684	457.537961	6.884070
6.315271	451.344549	6.889075
6.242845	457.322928	6.894080
6.157931	458.574349	6.899085
6.198693	448.680580	6.904090
6.213496	458.626612	6.909094
6.369925	449.557705	6.914099
6.268979	455.287621	6.919104
6.356281	461.160812	6.924109
6.351440	459.007509	6.929114
6.185040	459.092733	6.934118
6.331214	463.965931	6.939123
6.211361	458.076907	6.944128
6.468924	460.988463	6.949133
6.473947	455.714587	6.954138
6.111079	459.163622	6.959142
6.236585	459.239580	6.964147
6.156935	456.350159	6.969152
6.387576	463.622823	6.974157
6.590516	449.593404	6.979162
6.225324	457.842101	6.984166
5.861399	455.543424	6.989171
6.295281	452.386031	6.994176
6.231392	455.974803	6.999181
6.383423	451.972508	7.004186
6.467355	456.560594	7.009190
5.808821	451.335625	7.014195
6.240613	451.984256	7.019200
6.191968	457.401215	7.024205
6.405941	451.581434	7.029210
6.333455	464.360909	7.034214
5.986374	452.518308	7.039219
6.396514	445.388079	7.044224
5.964572	445.484123	7.049229
6.239347	451.077225	7.054234
6.072308	462.996567	7.059238
6.093343	458.066763	7.064243
6.269125	456.744933	7.069248
6.149809	468.259330	7.074253
6.331544	459.833894	7.079258
6.119748	459.996493	7.084262
5.904686	457.438726	7.089267
6.152176	451.644772	7.094272
6.028599	458.429659	7.099277
6.214393	448.329729	7.104282
6.017587	455.499712	7.109286
6.003503	447.856793	7.114291
6.356534	446.407536	7.119296
5.833700	443.292144	7.124301
6.147398	447.111040	7.129306
5.717416	452.228239	7.134310
5.884288	451.942138	7.139315
5.994066	462.747445	7.144320
6.205149	454.275118	7.149325
6.367486	455.748056	7.154330
6.321118	464.426453	7.159334
6.287760	457.546476	7.164339
6.134255	459.185384	7.169344
6.245335	455.555735	7.174349
6.241871	447.800944	7.179354
5.962189	460.065729	7.184358
6.089431	461.026464	7.189363
6.269772	454.395072	7.194368
5.925216	465.250555	7.199373
6.496037	457.211608	7.204378
5.985239	463.023407	7.209382
6.255202	457.053058	7.214387
6.500719	451.054001	7.219392
6.439591	466.755169	7.224397
6.445319	463.289193	7.229402
6.310415	460.071867	7.234406
6.171757	459.988113	7.239411
6.215333	450.623928	7.244416
6.217988	462.997860	7.249421
6.234240	457.006178	7.254426
6.001815	455.829698	7.259430
6.291398	454.965202	7.264435
6.046894	465.059360	7.269440
5.854450	458.270849	7.274445
5.939003	450.412481	7.279450
6.123002	451.340926	7.284454
6.181575	449.613044	7.289459
6.254844	462.049086	7.294464
6.069916	458.250790	7.299469
6.130720	459.214831	7.304474
5.969612	463.426717	7.309478
6.144187	462.974365	7.314483
6.203516	476.399421	7.319488
6.114416	483.672549	7.324493
6.556349	480.141045	7.329498
6.833672	461.742644	7.334502
6.218391	463.522748	7.339507
6.078603	458.439997	7.344512
6.343446	450.640773	7.349517
6.264828	446.826651	7.354522
6.206541	454.069996	7.359526
6.570142	453.861629	7.364531
6.293182	446.663433	7.369536
6.067166	461.979661	7.374541
6.330369	457.942773	7.379546
6.462172	458.065641	7.384550
6.187417	455.195703	7.389555
6.308996	451.635556	7.394560
6.132897	453.315107	7.399565
6.275665	453.121602	7.404570
6.173404	454.133958	7.409574
6.298912	451.011845	7.414579
6.503214	456.968276	7.419584
6.212350	451.023903	7.424589
6.356202	463.248155	7.429594
6.396563	458.117023	7.434598
6.382171	451.261733	7.439603
6.151800	436.746402	7.444608
5.955978	431.240571	7.449613
6.525110	433.110874	7.454618
6.336921	441.604354	7.459622
6.194105	431.522937	7.464627
6.320336	426.345823	7.469632
6.035150	430.333746	7.474637
5.948865	425.353839	7.479642
6.007295	425.440313	7.484646
6.220976	449.142628	7.489651
6.220178	452.367517	7.494656
6.235719	443.619137	7.499661
6.570912	426.695378	7.504666
6.175753	431.454753	7.509670
6.078808	430.803454	7.514675
6.089245	418.922791	7.519680
5.777912	436.003907	7.524685
6.267841	433.567390	7.529690
6.042597	449.312491	7.534694
6.372865	452.313438	7.539699
6.526458	452.336989	7.544704
5.927877	447.349359	7.549709
6.336416	446.798667	7.554714
6.036977	436.910327	7.559718
6.088516	434.655929	7.564723
6.592147	445.974205	7.569728
6.168013	432.639870	7.574733
6.263481	431.893560	7.579738
5.929279	430.257363	7.584742
5.820475	440.542949	7.589747
6.368115	441.741717	7.594752
6.337799	451.981949	7.599757
6.313721	445.741989	7.604762
6.172325	450.764630	7.609766
6.179770	441.819661	7.614771
6.474604	426.288100	7.619776
6.218447	427.513806	7.624781
6.190542	428.349859	7.629786
6.303416	419.445264	7.634790
6.051103	425.073741	7.639795
6.368780	426.060759	7.644800
5.984104	437.307676	7.649805
6.148128	433.029494	7.654810
6.286631	428.113794	7.659814
6.133347	420.790343	7.664819
5.944919	427.728829	7.669824
6.030070	438.458867	7.674829
6.208623	445.720019	7.679834
6.045900	454.615412	7.684838
6.282273	457.676902	7.689843
6.393124	453.434949	7.694848
5.944709	464.429191	7.699853
6.567386	458.350112	7.704858
6.300064	451.248592	7.709862
5.960972	442.000865	7.714867
6.171161	445.429002	7.719872
6.405886	454.822178	7.724877
6.557431	437.815348	7.729882
6.273905	423.310016	7.734886
6.270129	426.892971	7.739891
6.461353	424.222936	7.744896
6.223424	417.005266	7.749901
6.195349	425.128854	7.754906
6.139576	423.770383	7.759910
6.062155	419.740971	7.764915
6.504519	414.597353	7.769920
5.897507	420.148401	7.774925
5.977122	431.915970	7.779930
6.269257	420.472531	7.784934
5.578647	421.668551	7.789939
5.991313	428.924080	7.794944
6.212433	445.189841	7.799949
6.416236	449.985607	7.804954
6.119289	445.268308	7.809958
5.962866	448.133960	7.814963
6.386575	451.442279	7.819968
6.209256	453.372060	7.824973
6.212951	446.274800	7.829978
6.042195	438.260983	7.834982
6.120829	453.433018	7.839987
6.213020	454.455404	7.844992
6.486623	457.670178	7.849997
6.177888	446.846802	7.855002
6.261672	443.350342	7.860006
5.993144	445.426061	7.865011
6.390650	441.780756	7.870016
6.141445	444.617173	7.875021
6.336965	435.118905	7.880026
6.029549	427.092006	7.885030
6.086143	436.031979	7.890035
6.290002	451.287272	7.895040
6.084417	464.089379	7.900045
6.244256	454.007754	7.905050
6.312938	450.065637	7.910054
6.134896	458.523503	7.915059
6.112369	450.572357	7.920064
5.948538	455.713961	7.925069
6.368304	451.255484	7.930074
6.492352	458.335828	7.935078
6.176951	453.776888	7.940083
6.167451	429.602952	7.945088
6.209579	441.287933	7.950093
5.925741	437.800450	7.955098
6.059699	458.305086	7.960102
6.100365	458.782667	7.965107
6.558454	454.099981	7.970112
6.345171	461.627707	7.975117
6.306182	437.715182	7.980122
6.202810	435.986391	7.985139
5.947363	432.028262	7.990157
6.495459	432.012539	7.995174
5.935056	438.125193	8.000192
6.019572	447.232586	8.005210
6.091947	448.915398	8.010227
6.104628	452.433349	8.015245
6.347146	449.409015	8.020262
6.002462	456.664604	8.025280
6.152567	452.136791	8.030298
6.225510	467.302341	8.035315
6.252430	461.040530	8.040333
6.215197	452.211984	8.045350
6.013753	452.809124	8.050368
6.251779	457.546947	8.055386
6.376361	454.078595	8.060403
6.280104	454.674851	8.065421
6.422786	448.962729	8.070438
6.219179	464.631124	8.075456
6.202181	455.104396	8.080474
6.412810	457.047364	8.085491
6.559260	466.982440	8.090509
6.559353	453.236076	8.095526
6.698298	457.967868	8.100544
6.383590	454.228389	8.105562
6.602542	433.999051	8.110579
5.987009	432.481468	8.115597
6.116146	434.860730	8.120614
6.040821	454.104049	8.125632
6.565054	449.764460	8.130650
6.250678	447.434662	8.135667
6.181650	452.037715	8.140685
6.391549	451.260342	8.145702
6.378293	462.840242	8.150720
5.872794	460.990877	8.155738
6.179111	459.792253	8.160755
5.901529	461.958380	8.165773
6.301928	447.304654	8.170790
5.923983	451.088851	8.175808
5.905420	459.234262	8.180826
5.865303	471.987031	8.185843
6.036230	487.865455	8.190861
6.404161	480.649201	8.195878
6.366704	487.460060	8.200896
6.091652	488.661276	8.205914
6.495136	492.920760	8.210931
6.252646	500.247825	8.215949
6.265681	493.347993	8.220966
6.250407	493.959775	8.225984
6.440007	491.108357	8.231002
6.591955	492.075884	8.236019
6.336364	490.884094	8.241037
6.568503	487.967763	8.246054
6.419713	498.672563	8.251072
6.550756	494.339022	8.256090
6.643733	494.770488	8.261107
6.369980	499.740110	8.266125
6.286568	498.723336	8.271142
6.461646	500.983000	8.276160
6.439477	496.422289	8.281178
6.527588	491.158527	8.286195
6.233489	493.168743	8.291213
6.264913	491.236956	8.296230
6.420609	502.462751	8.301248
6.541540	512.176705	8.306266
6.731139	519.845189	8.311283
6.644064	522.785821	8.316301
6.658687	515.711713	8.321318
6.625710	502.028258	8.326336
6.275293	495.338404	8.331354
6.687310	496.869316	8.336371
6.701019	506.479377	8.341389
6.372733	489.844859	8.346406
6.608451	493.937060	8.351424
6.641782	509.835143	8.356442
6.551910	489.600183	8.361459
6.538699	490.274021	8.366477
6.800687	493.130467	8.371494
6.644858	487.088461	8.376512
6.547931	496.031849	8.381530
6.460734	493.100489	8.386547
6.411117	496.977953	8.391565
6.839390	502.886166	8.396582
6.861733	507.382379	8.401600
6.772157	499.449219	8.406618
6.608984	484.771667	8.411635
6.377907	485.324507	8.416653
6.509031	487.881781	8.421670
6.755534	495.394581	8.426688
6.514465	507.260843	8.431706
6.565401	500.629514	8.436723
6.517113	512.375477	8.441741
6.766524	511.338428	8.446758
6.768573	518.214997	8.451776
6.625979	513.794687	8.456794
6.496626	519.274812	8.461811
6.682753	509.572888	8.466829
6.760777	522.141778	8.471846
6.436582	517.477543	8.476864
6.529110	515.719480	8.481882
6.854575	509.099376	8.486899
6.786430	524.474552	8.491917
6.891309	516.434779	8.496934
6.601049	518.366219	8.501952
6.573720	516.205593	8.506970
6.415778	520.058288	8.511987
6.690964	525.549766	8.517005
6.838306	513.095997	8.522022
6.742710	525.759777	8.527040
6.803654	511.294675	8.532058
7.115577	514.355242	8.537075
6.484975	517.496895	8.542093
6.823796	521.239771	8.547110
6.755274	517.106976	8.552128
6.544440	525.874375	8.557146
6.885103	513.439179	8.562163
6.739287	536.849287	8.567181
6.576768	524.049605	8.572199
6.740558	516.318360	8.577216
6.544557	528.749575	8.582234
6.959248	516.986320	8.587251
6.801175	529.962200	8.592269
6.807804	521.294252	8.597287
6.814170	520.035657	8.602304
6.521857	525.077253	8.607322
6.611465	531.569276	8.612339
6.795779	555.852434	8.617357
6.661172	553.355655	8.622375
6.544197	559.204585	8.627392
6.825337	559.181302	8.632410
7.139294	546.409777	8.637427
7.172266	550.421403	8.642445
6.819681	552.434226	8.647463
7.326364	554.925580	8.652480
6.961566	557.912208	8.657498
7.197727	555.276478	8.662515
7.154244	534.242299	8.667533
7.013946	528.254984	8.672551
6.887429	525.611999	8.677568
6.772457	525.239379	8.682586
6.803554	521.253854	8.687603
6.831290	523.317465	8.692621
6.920052	541.609967	8.697639
6.796636	542.555582	8.702656
7.120282	552.079704	8.707674
7.276158	548.370732	8.712691
6.696714	544.761875	8.717709
6.736089	550.865599	8.722727
7.379619	550.967725	8.727744
7.143399	546.243838	8.732762
7.094567	525.025334	8.737779
6.889397	518.518292	8.742797
6.644058	533.667328	8.747815
7.210296	538.041398	8.752832
6.839133	551.626754	8.757850
7.209215	550.718331	8.762867
6.946469	556.540616	8.767885
7.270942	550.148398	8.772903
7.138263	547.597368	8.777920
7.106708	550.566210	8.782938
7.242311	540.917709	8.787955
7.022726	534.257350	8.792973
7.011593	524.769762	8.797991
7.042710	524.260360	8.803008
6.956674	528.175554	8.808026
7.202121	545.258735	8.813043
7.255873	552.527713	8.818061
6.952895	539.302294	8.823079
7.176789	532.304343	8.828096
7.242933	537.055104	8.833114
7.304511	521.629325	8.838131
6.889744	519.364366	8.843149
6.934278	524.345063	8.848167
7.339650	535.627364	8.853184
7.283786	544.189990	8.858202
7.647299	530.602456	8.863219
7.382038	524.617333	8.868237
7.292893	518.898894	8.873255
7.263291	522.731714	8.878272
7.201908	518.938460	8.883290
7.499269	521.431796	8.888307
7.283443	519.274630	8.893325
7.293158	515.492829	8.898343
7.668749	516.119605	8.903360
7.521854	522.357700	8.908378
7.368739	513.795928	8.913395
7.333325	509.223825	8.918413
7.335534	509.483722	8.923431
7.523257	503.740304	8.928448
7.022978	501.626703	8.933466
7.158113	485.994502	8.938483
7.328307	499.160072	8.943501
6.902114	504.007114	8.948519
7.098780	502.244602	8.953536
6.994454	513.472522	8.958554
6.676017	517.613979	8.963571
7.062486	512.274820	8.968589
6.933581	512.612921	8.973607
7.091115	516.273029	8.978624
6.827643	525.426677	8.983642
6.797548	524.907728	8.988659
7.420717	546.297732	8.993677
7.577265	556.553218	8.998695
7.573423	547.812979	9.003712
7.440460	553.660420	9.008730
7.553364	533.462883	9.013747
7.102742	529.422490	9.018765
7.101013	529.910780	9.023783
7.636180	527.815655	9.028800
7.603418	526.875131	9.033818
7.352003	519.034504	9.038835
7.476807	520.011646	9.043853
7.070575	524.257597	9.048871
7.180503	521.317997	9.053888
7.388916	540.645136	9.058906
7.457735	540.384787	9.063923
7.571264	542.508204	9.068941
7.446727	541.965527	9.073959
7.354239	527.287646	9.078976
7.256436	540.744857	9.083994
7.729359	535.740561	9.089011
7.702565	528.944742	9.094029
7.270033	524.587401	9.099047
7.500780	519.956851	9.104064
7.201910	519.950487	9.109082
7.270560	527.597275	9.114099
7.466353	537.676970	9.119117
7.433161	554.918500	9.124135
7.644097	542.691364	9.129152
7.591460	550.826522	9.134170
7.486350	542.204819	9.139187
7.400825	540.245152	9.144205
7.449057	552.692434	9.149223
7.691283	539.594432	9.154240
7.470466	550.417290	9.159258
7.490948	553.590492	9.164275
7.703511	550.055978	9.169293
7.242235	542.075892	9.174311
7.471727	550.502298	9.179328
7.388058	555.294013	9.184346
7.510257	551.931144	9.189363
7.577083	548.316243	9.194381
7.347096	564.427659	9.199399
7.428248	561.420380	9.204416
7.331724	553.813911	9.209434
7.466107	548.564906	9.214451
7.331292	553.393828	9.219469
7.457100	557.950083	9.224487
7.665113	552.383392	9.229504
7.610184	553.154883	9.234522
7.454690	560.947457	9.239539
7.630543	555.976602	9.244557
7.631671	551.500003	9.249575
7.659016	552.242909	9.254592
7.477757	550.623677	9.259610
7.527500	546.436646	9.264627
7.900531	550.623045	9.269645
7.581139	563.222348	9.274663
8.014762	561.346382	9.279680
7.712714	553.402714	9.284698
7.837653	555.451610	9.289715
7.887102	553.941013	9.294733
7.866923	556.885533	9.299751
7.722597	550.943165	9.304768
7.636592	561.186068	9.309786
7.691376	555.417405	9.314803
7.792569	549.458000	9.319821
7.243811	554.814297	9.324839
7.640473	548.695932	9.329856
7.735064	553.374866	9.334874
7.564771	546.615400	9.339891
8.016796	549.371102	9.344909
7.819548	552.214047	9.349927
7.691185	550.454175	9.354944
7.780320	557.345078	9.359962
7.784286	556.537240	9.364979
7.922045	551.910466	9.369997
7.578201	560.439890	9.375015
7.729225	544.958728	9.380032
7.714040	556.591179	9.385050
7.665582	550.425667	9.390067
7.648301	547.384891	9.395085
7.502930	565.338661	9.400103
7.862691	574.332049	9.405120
8.153292	575.913782	9.410138
8.041765	573.188784	9.415155
8.025165	555.729012	9.420173
7.753746	558.434448	9.425191
7.738824	553.730995	9.430208
7.704160	552.485097	9.435226
7.948692	566.810773	9.440243
7.815856	570.236321	9.445261
7.807305	582.335574	9.450279
7.976405	587.597611	9.455296
7.638828	587.588209	9.460314
7.712059	580.962799	9.465331
7.988389	582.173102	9.470349
7.860209	583.642504	9.475367
7.896772	578.069749	9.480384
7.961494	587.524179	9.485402
7.643117	580.097930	9.490419
7.611247	584.180337	9.495437
7.799494	589.757096	9.500455
7.821653	584.651260	9.505472
7.753097	592.043260	9.510490
7.782741	595.041344	9.515507
7.632751	588.119847	9.520525
7.607622	592.187952	9.525543
7.886955	613.710573	9.530560
8.022158	620.607851	9.535578
8.048528	629.522237	9.540595
7.906047	621.423181	9.545613
7.668613	620.128577	9.550631
7.866006	617.266201	9.555648
7.930190	631.681641	9.560666
7.666298	634.775582	9.565683
8.145705	627.918531	9.570701
8.086015	630.802093	9.575719
8.145040	630.083356	9.580736
8.158779	628.491860	9.585754
7.904648	633.689558	9.590771
7.892593	626.874132	9.595789
8.199884	625.481647	9.600807
8.300399	635.211066	9.605824
8.491608	622.913123	9.610842
8.236253	631.241330	9.615859
8.413337	628.231734	9.620877
8.349034	629.498055	9.625895
8.082204	622.380748	9.630912
8.489813	620.716353	9.635930
8.256325	627.787082	9.640947
8.343190	620.905674	9.645965
8.206729	628.227642	9.650983
8.227245	617.642702	9.656000
8.499867	611.085829	9.661018
8.082279	605.439265	9.666035
8.170643	591.504748	9.671053
7.934116	600.312465	9.676071
8.304146	611.915220	9.681088
8.278350	622.414121	9.686106
8.015689	628.742093	9.691123
8.424585	622.895868	9.696141
8.114212	624.059836	9.701159
8.229409	623.337703	9.706176
8.360042	626.958987	9.711194
8.296858	629.717742	9.716211
8.679817	616.952252	9.721229
8.182639	598.659475	9.726247
8.345633	591.499744	9.731264
8.330489	592.869724	9.736282
7.834249	590.688910	9.741299
8.001647	606.179286	9.746317
8.039492	617.789420	9.751335
7.983699	619.231091	9.756352
8.074164	624.744139	9.761370
8.068953	621.902321	9.766387
8.721472	624.330366	9.771405
8.303919	627.874723	9.776423
8.127072	625.945324	9.781440
8.330096	627.938389	9.786458
8.225785	630.855716	9.791475
8.333859	626.900327	9.796493
8.500494	624.104653	9.801511
8.618933	632.177667	9.806528
8.464248	622.806108	9.811546
8.498352	625.420807	9.816563
8.508791	627.873491	9.821581
8.143215	630.440604	9.826599
8.280661	626.926582	9.831616
8.651163	623.472583	9.836634
8.291429	629.618218	9.841651
8.588322	620.073856	9.846669
8.781845	625.945798	9.851687
8.366121	634.050186	9.856704
8.654350	614.044953	9.861722
8.313153	622.067116	9.866739
8.531561	621.790852	9.871757
8.548579	627.024942	9.876775
8.489312	623.848396	9.881792
8.794539	620.164869	9.886810
8.220035	620.538969	9.891827
8.746929	628.115237	9.896845
8.625010	629.341496	9.901863
8.426282	626.457908	9.906880
8.766960	623.567079	9.911898
8.181688	628.143278	9.916915
8.654877	618.595902	9.921933
8.742259	626.550639	9.926951
8.379904	626.466998	9.931968
8.307530	620.838258	9.936986
8.373277	625.552303	9.942003
8.283108	614.054456	9.947021
8.543658	624.832099	9.952039
8.221135	627.191899	9.957056
8.428715	622.919856	9.962074
8.816459	645.298329	9.967091
8.940001	640.221156	9.972109
8.683901	629.276135	9.977127
8.511169	628.123169	9.982144
8.900245	623.302404	9.987162
8.427796	624.277477	9.992179
8.565363	618.030349	9.997197
8.727088	629.049542	10.002215
8.720676	624.840886	10.007232
8.836955	626.622739	10.012250
8.428172	628.354346	10.017267
8.590477	647.738070	10.022285
8.814022	645.096934	10.027303
8.807388	641.861672	10.032320
9.145379	643.680037	10.037338
8.726004	627.352364	10.042355
8.643171	623.863404	10.047373
8.886170	620.114989	10.052391
8.132612	627.857432	10.057408
8.546446	630.785800	10.062426
8.552862	642.841089	10.067443
8.926759	654.643814	10.072461
8.981157	652.647576	10.077479
8.815765	648.022945	10.082496
9.151210	643.819284	10.087514
8.779595	648.202244	10.092531
8.913876	650.122055	10.097549
8.977953	646.210952	10.102567
8.444157	636.223665	10.107584
8.810765	645.045499	10.112602
8.529087	655.643484	10.117619
8.332893	651.788865	10.122637
8.441397	641.126350	10.127655
8.399864	653.156125	10.132672
8.633343	654.588280	10.137690
8.820931	654.150989	10.142707
8.696784	640.903545	10.147725
8.629953	648.549994	10.152743
8.803551	671.860761	10.157760
9.028734	676.620463	10.162778
8.817970	686.552829	10.167795
8.882931	681.621161	10.172813
8.511039	684.831416	10.177831
8.620282	686.437681	10.182848
8.900316	681.081445	10.187866
8.915763	685.509762	10.192883
8.689600	680.205070	10.197901
8.781688	680.072945	10.202919
8.971863	680.179678	10.207936
8.974664	675.717333	10.212954
9.157127	684.641333	10.217971
9.104782	683.089120	10.222989
9.117998	684.841199	10.228007
9.057117	689.210508	10.233024
9.019410	682.692396	10.238042
9.083645	675.991669	10.243059
9.189662	684.716924	10.248077
9.239275	674.991246	10.253095
9.034763	683.100642	10.258112
8.931037	677.160359	10.263130
9.161329	676.092019	10.268147
9.185736	680.648763	10.273165
9.164177	672.615478	10.278183
9.113210	683.319362	10.283200
9.123277	677.728323	10.288218
9.195272	681.903195	10.293235
9.047906	686.940721	10.298253
9.275601	682.793078	10.303271
9.272451	689.897539	10.308288
9.133720	678.026804	10.313306
9.189794	687.836643	10.318323
9.289760	682.143319	10.323341
9.272389	679.237367	10.328359
9.439424	690.499213	10.333376
9.596672	688.222964	10.338394
9.516929	682.281464	10.343411
9.458273	679.136300	10.348429
9.072695	685.230138	10.353447
8.926525	680.168090	10.358464
9.484812	679.708779	10.363482
9.220244	687.330515	10.368499
9.308976	682.082725	10.373517
9.325773	675.857541	10.378535
8.938258	686.481734	10.383552
9.037366	681.769201	10.388570
9.265087	683.957384	10.393587
9.279543	686.699355	10.398605
9.389537	680.472908	10.403623
8.961154	679.706149	10.408640
9.377169	677.102029	10.413658
9.246070	675.660883	10.418675
9.083857	676.736938	10.423693
9.429586	670.976938	10.428711
9.275830	679.321612	10.433728
9.354378	681.854556	10.438746
9.301134	680.388707	10.443763
9.221393	676.040417	10.448781
9.499129	675.761415	10.453799
9.054890	685.948572	10.458816
9.495400	678.743828	10.463834
9.462619	675.918376	10.468851
9.173861	675.248568	10.473869
9.324736	675.613762	10.478887
9.070737	679.972530	10.483904
9.254320	690.704898	10.488922
9.260943	697.345567	10.493939
9.245218	712.346130	10.498957
9.496215	707.956448	10.503975
9.220557	708.475341	10.508992
9.500180	712.350107	10.514010
9.472631	710.522148	10.519027
9.361348	715.714328	10.524045
9.413065	708.856613	10.529063
9.251152	714.259133	10.534080
9.277446	708.945694	10.539098
9.816693	713.110125	10.544115
9.518755	712.004065	10.549133
9.686326	703.328851	10.554151
9.731672	721.742332	10.559168
9.571675	712.448956	10.564186
9.723325	713.552168	10.569203
9.339149	718.159261	10.574221
9.578452	719.375904	10.579239
9.699230	710.517107	10.584256
9.885188	717.654041	10.589274
9.834266	711.713662	10.594291
9.351108	719.667263	10.599309
9.724865	717.341377	10.604327
9.854883	714.564939	10.609344
9.652468	710.890852	10.614362
9.665464	718.712294	10.619379
9.400031	713.619593	10.624397
9.638419	713.034132	10.629415
9.852493	713.589244	10.634432
9.419459	717.315899	10.639450
9.631988	724.992891	10.644467
9.661533	725.271099	10.649485
9.836461	713.099592	10.654503
9.539375	718.990612	10.659520
9.572969	707.397205	10.664538
9.696537	713.756721	10.669555
9.524123	715.945031	10.674573
9.772304	709.128401	10.679591
9.853661	708.361476	10.684608
9.816920	714.404646	10.689626
9.629093	711.258820	10.694643
9.679155	717.426978	10.699661
9.995161	706.659195	10.704679
9.838328	714.882357	10.709696
9.466240	712.967366	10.714714
9.922779	709.529020	10.719731
9.593066	729.471853	10.724749
10.046214	742.646480	10.729767
9.725539	737.739287	10.734784
9.730823	751.508527	10.739802
10.202323	748.033446	10.744819
9.834187	742.042441	10.749837
10.090324	724.127890	10.754855
9.648009	723.428786	10.759872
9.716303	740.541322	10.764890
9.937602	741.943220	10.769907
10.011914	745.794516	10.774925
10.140364	745.394967	10.779943
10.202767	741.471126	10.784960
9.788598	732.232032	10.789978
9.959753	721.633492	10.794995
9.872247	734.150048	10.800013
10.189474	727.906587	10.805031
9.778769	730.951241	10.810048
9.808775	742.963333	10.815066
10.094348	743.562902	10.820083
9.726174	755.161048	10.825101
10.050825	753.926298	10.830119
9.734977	751.585871	10.835136
9.827138	754.211842	10.840154
9.796767	752.516227	10.845171
9.590228	750.627751	10.850189
9.683923	750.291434	10.855207
9.919781	756.409944	10.860224
9.767711	753.592027	10.865242
10.208370	760.508467	10.870259
9.780234	769.562367	10.875277
9.845696	775.028825	10.880295
10.137364	772.131518	10.885312
10.268389	784.722945	10.890330
10.215553	777.859286	10.895347
9.988803	790.654050	10.900365
10.467129	785.125187	10.905383
10.519666	777.981495	10.910400
10.139222	773.744388	10.915418
10.347768	760.999198	10.920435
9.978830	761.323316	10.925453
10.105192	762.173647	10.930471
10.102452	773.757746	10.935488
10.022551	774.431222	10.940506
10.390677	780.639644	10.945523
10.275573	768.349990	10.950541
10.147810	766.635857	10.955559
10.185112	774.287564	10.960576
10.038037	778.563302	10.965594
10.564415	768.760977	10.970611
10.535870	779.599003	10.975629
10.462422	773.683589	10.980647
10.278008	778.752475	10.985664
10.439118	776.998378	10.990682
10.285157	782.783048	10.995699
10.398744	786.415264	11.000717
10.375092	776.132789	11.005735
10.211748	773.502946	11.010752
10.401166	778.266239	11.015770
10.748975	773.184167	11.020787
10.198331	774.371005	11.025805
10.407103	768.934026	11.030823
10.258355	778.614463	11.035840
10.472540	782.827230	11.040858
10.453980	777.899521	11.045875
10.281914	774.777842	11.050893
10.683564	779.280413	11.055911
10.764973	776.204156	11.060928
10.782406	773.479026	11.065946
10.423999	760.076190	11.070963
10.621719	752.578959	11.075981
10.241926	749.266894	11.080999
10.331641	748.586767	11.086016
10.202353	753.963821	11.091034
10.460206	747.156595	11.096051
10.384158	774.186991	11.101069
10.371079	770.198482	11.106087
10.670569	765.330307	11.111104
10.480103	775.743594	11.116122
10.500623	773.760037	11.121139
10.176892	772.844455	11.126157
10.246659	772.745157	11.131175
10.657310	779.228804	11.136192
10.549120	774.952123	11.141210
10.784887	772.284140	11.146227
10.590759	773.900889	11.151245
10.618511	768.609234	11.156263
10.358184	772.352969	11.161280
10.092497	778.162044	11.166298
10.505423	771.316924	11.171315
10.139994	781.304489	11.176333
10.588547	791.562757	11.181351
10.661225	795.658811	11.186368
10.793263	807.672167	11.191386
10.774240	801.213901	11.196403
10.536347	795.510346	11.201421
10.688825	803.648085	11.206439
10.787697	803.119974	11.211456
10.601491	807.078202	11.216474
10.895163	813.259205	11.221491
10.739980	816.750118	11.226509
10.632447	807.333042	11.231527
10.711458	808.528600	11.236544
10.500796	812.884953	11.241562
10.831669	809.238274	11.246579
10.447551	812.158862	11.251597
10.526632	820.259947	11.256615
10.693115	815.147655	11.261632
10.564526	817.552332	11.266650
10.795467	809.447243	11.271667
10.512147	809.140288	11.276685
10.876853	818.618801	11.281703
11.101522	812.048526	11.286720
10.900956	816.087870	11.291738
11.121840	810.789808	11.296755
11.105059	810.177311	11.301773
10.741004	815.212968	11.306791
11.086415	809.939558	11.311808
10.867239	819.863561	11.316826
10.892232	808.234104	11.321843
11.019801	811.082162	11.326861
10.752058	808.847927	11.331879
10.907051	803.294652	11.336896
10.715663	810.960232	11.341914
10.723199	810.480709	11.346931
10.907092	820.427724	11.351949
10.853764	835.984605	11.356967
11.204716	839.528316	11.361984
11.070306	852.983789	11.367002
11.184829	827.785462	11.372019
11.242057	828.834244	11.377037
11.024878	820.431721	11.382055
11.040019	809.385360	11.387072
11.111502	810.192816	11.392090
11.036002	809.616813	11.397107
10.951891	818.262217	11.402125
10.874830	840.771090	11.407143
11.229979	848.793799	11.412160
11.434517	854.875017	11.417178
11.163891	844.258218	11.422195
11.105692	824.479954	11.427213
10.786058	827.555212	11.432231
10.884482	838.543504	11.437248
10.876690	847.262108	11.442266
11.185451	854.806700	11.447283
10.931007	844.535234	11.452301
10.670587	849.055734	11.457319
11.201072	844.827594	11.462336
11.137332	851.295345	11.467354
10.980386	841.839189	11.472371
11.184714	846.645308	11.477389
11.188818	849.452011	11.482407
11.310852	841.560993	11.487424
10.965836	853.449849	11.492442
11.626589	844.056306	11.497459
11.307055	849.210579	11.502477
11.162767	851.174970	11.507495
11.360873	840.862817	11.512512
11.033947	848.930368	11.517530
11.283121	859.099657	11.522547
11.268757	869.807056	11.527565
11.298318	878.350603	11.532583
11.769328	871.482043	11.537600
11.391132	863.195133	11.542618
11.380424	857.207883	11.547635
11.456193	849.607579	11.552653
11.344750	848.982805	11.557671
11.661494	858.459049	11.562688
11.524565	851.185289	11.567706
11.176550	848.491924	11.572723
11.539876	854.644874	11.577741
11.614288	853.564542	11.582759
11.369562	848.330579	11.587776
11.547204	848.305538	11.592794
11.814941	841.508839	11.597811
11.653376	841.918297	11.602829
11.291643	843.751381	11.607847
11.502439	839.075814	11.612864
11.467463	842.444077	11.617882
11.660261	841.131554	11.622899
11.757324	844.301583	11.627917
11.545158	843.284060	11.632935
11.788498	847.314074	11.637952
11.903768	854.453722	11.642970
11.989772	844.734903	11.647987
12.202999	847.215652	11.653005
11.660659	853.344569	11.658023
12.032487	859.369348	11.663040
11.953427	853.028870	11.668058
11.888108	838.302300	11.673075
11.867094	820.833905	11.678093
11.348565	822.126446	11.683111
11.729423	820.205648	11.688128
11.538730	815.340681	11.693146
11.602135	837.313324	11.698163
11.921771	831.250516	11.703181
11.693827	838.202516	11.708199
11.766203	839.568852	11.713216
11.774110	836.933473	11.718234
11.550502	844.646135	11.723251
11.790938	839.368840	11.728269
11.751221	846.733746	11.733287
12.027257	842.981185	11.738304
11.697279	839.413226	11.743322
11.625421	844.156030	11.748339
12.181771	840.905841	11.753357
11.633919	847.099445	11.758375
11.495008	837.729670	11.763392
11.839837	848.322853	11.768410
11.535546	842.174000	11.773427
11.553292	847.899160	11.778445
11.583295	847.484809	11.783463
11.741454	844.149386	11.788480
11.763432	848.243220	11.793498
11.855139	839.128547	11.798515
11.865141	833.955552	11.803533
11.414079	844.271100	11.808551
11.549035	846.127442	11.813568
11.746505	862.918343	11.818586
11.788253	875.309283	11.823603
12.126145	864.218492	11.828621
12.248547	880.315186	11.833639
12.120305	872.949037	11.838656
12.020594	881.005749	11.843674
12.304211	878.517217	11.848691
12.117604	865.866903	11.853709
11.970951	854.521334	11.858727
11.802044	855.217033	11.863744
11.950446	876.546554	11.868762
11.923892	873.528312	11.873779
12.115332	876.824445	11.878797
12.019451	884.815174	11.883815
12.084773	877.107930	11.888832
12.163680	879.417235	11.893850
12.073309	873.640800	11.898867
12.259683	874.731187	11.903885
11.956672	882.260176	11.908903
11.865591	873.415898	11.913920
11.987237	883.644902	11.918938
11.709348	875.425623	11.923955
11.685280	883.304071	11.928973
11.987933	875.879951	11.933991
12.108970	881.294726	11.939008
12.285768	892.112605	11.944026
12.053815	901.312038	11.949043
12.096266	900.844447	11.954061
12.174634	908.115421	11.959079
12.406958	904.929900	11.964096
12.250586	902.570521	11.969114
12.263590	897.312365	11.974131
12.439834	891.756720	11.979149
12.496346	902.498073	11.984167
12.309479	909.686598	11.989184
12.363179	896.000056	11.994202
12.399760	905.063296	11.999219
12.242666	898.380227	12.004237
12.167300	900.467851	12.009255
12.157120	897.823646	12.014272
12.071128	903.263263	12.019290
12.163876	900.538631	12.024307
12.498135	904.835873	12.029325
12.330099	913.774742	12.034343
12.315305	906.326014	12.039360
12.517955	900.925434	12.044378
12.293436	912.249526	12.049395
12.054914	907.494414	12.054413
11.908805	907.117887	12.059431
12.554868	926.045097	12.064448
12.886242	930.570373	12.069466
12.275174	934.046258	12.074483
12.570826	928.305480	12.079501
12.607430	934.783813	12.084519
12.575732	939.242843	12.089536
12.621573	940.012821	12.094554
12.525717	939.358692	12.099571
12.609920	926.313894	12.104589
12.860913	934.686951	12.109607
12.511638	921.784801	12.114624
12.882052	920.390499	12.119642
12.543265	911.680128	12.124659
13.017492	895.478789	12.129677
12.464284	908.827685	12.134695
12.491665	903.141970	12.139712
12.700591	905.445890	12.144730
12.350823	908.590718	12.149747
12.429462	926.288726	12.154765
12.473028	928.913326	12.159783
12.398111	936.058916	12.164800
12.769412	929.813900	12.169818
12.430043	935.053765	12.174835
12.601875	934.590730	12.179853
12.524719	935.884597	12.184871
12.539902	939.755968	12.189888
12.895366	929.138971	12.194906
12.220863	945.851533	12.199923
12.855014	948.084257	12.204941
12.682115	966.302288	12.209959
12.981077	972.441929	12.214976
13.106692	956.577771	12.219994
13.267594	944.944209	12.225011
13.169803	944.989975	12.230029
13.096657	932.876305	12.235047
12.992159	922.683495	12.240064
13.338199	930.808144	12.245082
12.820083	926.687488	12.250099
13.140694	933.814034	12.255117
13.189030	929.529500	12.260135
12.611238	931.993227	12.265152
13.040464	930.425413	12.270170
12.599621	938.958311	12.275187
13.148628	934.725900	12.280205
12.964836	928.329116	12.285223
12.590107	931.999317	12.290240
13.326943	929.423128	12.295258
12.640227	931.487983	12.300275
13.145384	929.944208	12.305293
12.940070	930.017621	12.310311
12.585798	939.030649	12.315328
13.020373	945.294272	12.320346
12.920746	964.698146	12.325363
13.258438	961.882550	12.330381
13.096743	958.662270	12.335399
13.097607	970.841957	12.340416
13.362771	959.658421	12.345434
13.478221	963.339580	12.350451
13.171556	954.089243	12.355469
12.932067	944.742358	12.360487
13.133655	960.715004	12.365504
12.922697	960.733842	12.370522
13.072060	971.363414	12.375539
13.264771	971.142186	12.380557
13.143144	968.096758	12.385575
13.299414	972.723874	12.390592
13.299956	967.222888	12.395610
13.326448	972.128964	12.400627
13.299785	971.825958	12.405645
13.437991	969.079219	12.410663
13.448236	971.189682	12.415680
13.317602	967.444594	12.420698
12.989163	973.973551	12.425715
12.873442	972.497942	12.430733
13.302616	969.095961	12.435751
12.999496	973.599552	12.440768
13.118887	965.890791	12.445786
13.396475	966.164934	12.450803
13.213715	964.579173	12.455821
13.408234	969.588520	12.460839
13.472005	990.049573	12.465856
13.344342	984.992627	12.470874
13.287122	997.518946	12.475891
13.528366	1001.541080	12.480909
13.839114	999.068114	12.485927
13.413058	998.582043	12.490944
13.580507	988.185502	12.495962
13.554390	993.431778	12.500979
13.306872	996.247893	12.505997
13.658381	998.956545	12.511015
13.521550	1004.283755	12.516032
13.909524	1004.336872	12.521050
13.519592	988.325386	12.526067
13.271594	993.782414	12.531085
13.635362	994.491480	12.536103
13.256159	1007.805742	12.541120
13.566702	1002.456549	12.546138
13.325121	1011.260020	12.551155
13.440600	999.277655	12.556173
13.767471	998.834218	12.561191
13.663137	1013.256069	12.566208
13.526523	1000.403280	12.571226
13.535164	1010.361723	12.576243
13.535581	1008.873965	12.581261
13.490433	1003.747445	12.586279
13.540945	1007.960213	12.591296
13.672334	1009.168767	12.596314
13.666508	1018.096187	12.601331
14.002857	1020.823888	12.606349
13.978024	1021.573686	12.611367
13.813908	1016.283799	12.616384
14.027834	1000.495126	12.621402
13.906796	1004.523318	12.626419
13.942563	1002.389969	12.631437
14.176123	997.972780	12.636455
13.693908	997.784579	12.641472
13.737920	999.733554	12.646490
13.667688	1001.055412	12.651507
13.902846	1003.461692	12.656525
14.161382	1008.060468	12.661543
14.024271	1000.741394	12.666560
13.962801	1006.955694	12.671578
13.969664	1006.220382	12.676595
13.867288	1009.706137	12.681613
13.983282	1005.870201	12.686631
14.039604	1005.424718	12.691648
13.880079	1013.578802	12.696666
14.230058	1015.737338	12.701683
14.014186	1020.331216	12.706701
13.979118	1012.044884	12.711719
14.027614	1031.107003	12.716736
14.114363	1026.317675	12.721754
14.095100	1033.609993	12.726771
14.189817	1024.716752	12.731789
14.231990	1028.813982	12.736807
13.837329	1027.934931	12.741824
13.950132	1033.076724	12.746842
14.149446	1028.590790	12.751859
14.153526	1026.015459	12.756877
14.334735	1018.996800	12.761895
14.141561	1026.813957	12.766912
14.360612	1028.760722	12.771930
14.641031	1031.125260	12.776947
14.248336	1023.757951	12.781965
14.456269	1019.919386	12.786983
14.101332	1008.578275	12.792000
14.432407	1008.143197	12.797018
14.222855	1019.416071	12.802035
14.243517	1027.100578	12.807053
14.437393	1022.883646	12.812071
14.409297	1025.071328	12.817088
14.082973	1010.540565	12.822106
14.422585	1017.252210	12.827123
14.046959	1025.144065	12.832141
14.464338	1024.318726	12.837159
14.063764	1032.078108	12.842176
14.148404	1025.702184	12.847194
13.735035	1023.525102	12.852211
14.002615	1033.864679	12.857229
14.345371	1031.029335	12.862247
13.972176	1035.239049	12.867264
14.344279	1045.316847	12.872282
14.614219	1048.894101	12.877299
14.376973	1059.096434	12.882317
14.478193	1053.420089	12.887335
14.343932	1056.763108	12.892352
14.178547	1053.394213	12.897370
14.685260	1053.326097	12.902387
14.178079	1056.218291	12.907405
14.417887	1055.084966	12.912423
14.464080	1062.018047	12.917440
14.433149	1065.950627	12.922458
14.478477	1062.080713	12.927475
14.332711	1067.874367	12.932493
14.278378	1064.550857	12.937511
14.786405	1075.241575	12.942528
14.724225	1087.313686	12.947546
14.621635	1090.167627	12.952563
14.413991	1093.449581	12.957581
14.615186	1082.288361	12.962599
14.642016	1087.958169	12.967616
14.949208	1084.182676	12.972634
14.940649	1087.370639	12.977651
14.907230	1092.203606	12.982669
14.855957	1088.388263	12.987687
14.905875	1094.138499	12.992704
14.922756	1088.743815	12.997722
14.877113	1090.423013	13.002739
14.732820	1097.172306	13.007757
14.822880	1086.091689	13.012775
15.116549	1097.707258	13.017792
15.045937	1091.634172	13.022810
14.754396	1082.097012	13.027827
14.698601	1091.189043	13.032845
15.276525	1086.187264	13.037863
14.779997	1083.134605	13.042880
14.957987	1097.570410	13.047898
15.005100	1094.184821	13.052915
14.743209	1083.073908	13.057933
15.038287	1083.947498	13.062951
14.683243	1092.529261	13.067968
14.475503	1091.494848	13.072986
14.843039	1089.049471	13.078003
14.725541	1089.944927	13.083021
14.966065	1083.265617	13.088039
14.832872	1085.947466	13.093056
14.962780	1088.125527	13.098074
15.245129	1092.029858	13.103091
15.199529	1100.974149	13.108109
14.932372	1090.191256	13.113127
15.227883	1106.347705	13.118144
15.028416	1100.109346	13.123162
15.435684	1104.724858	13.128179
15.186307	1110.671901	13.133197
15.107915	1086.742460	13.138215
15.649422	1090.699935	13.143232
15.120357	1090.724207	13.148250
15.120549	1088.939246	13.153267
14.885209	1090.514822	13.158285
15.270616	1102.113628	13.163303
15.561051	1108.430320	13.168320
15.521576	1107.138916	13.173338
15.497395	1099.886525	13.178355
15.141828	1089.178508	13.183373
15.311469	1084.706920	13.188391
15.336552	1081.228528	13.193408
15.168387	1093.864632	13.198426
15.546380	1104.585565	13.203443
15.481843	1118.634795	13.208461
15.485985	1119.790415	13.213479
15.711472	1104.338687	13.218496
15.561649	1089.184155	13.223514
15.458931	1094.780540	13.228531
15.341815	1092.546122	13.233549
15.544657	1083.992016	13.238567
15.644717	1089.955988	13.243584
15.141385	1087.329637	13.248602
15.280382	1095.818962	13.253619
15.329607	1111.864630	13.258637
15.818922	1118.716483	13.263655
15.841983	1122.765724	13.268672
15.607822	1120.321164	13.273690
15.824421	1120.886503	13.278707
15.296762	1114.954838	13.283725
15.920493	1118.648713	13.288743
16.156354	1108.199820	13.293760
15.357020	1097.271592	13.298778
15.753211	1084.883634	13.303795
15.340917	1094.138634	13.308813
15.537240	1108.212765	13.313831
15.637757	1117.308847	13.318848
15.401303	1117.700792	13.323866
15.745645	1119.162663	13.328883
15.357578	1132.511962	13.333901
15.880380	1124.646952	13.338919
15.798540	1125.704216	13.343936
15.686107	1124.345367	13.348954
15.853818	1127.260850	13.353971
15.745246	1132.164540	13.358989
15.883233	1119.870097	13.364007
15.865527	1121.934816	13.369024
15.645751	1122.877131	13.374042
15.750074	1119.831263	13.379059
15.683950	1121.941401	13.384077
15.686013	1122.740291	13.389095
15.910143	1128.471140	13.394112
15.489713	1125.190918	13.399130
15.817730	1138.316921	13.404147
15.979952	1152.419966	13.409165
16.177854	1152.306928	13.414183
16.098577	1148.525734	13.419200
15.692537	1158.186023	13.424218
16.138750	1143.959870	13.429235
16.091278	1155.741419	13.434253
16.075735	1153.890554	13.439271
16.278498	1148.963477	13.444288
15.872381	1155.871896	13.449306
16.084783	1154.189577	13.454323
16.028570	1153.713907	13.459341
15.992904	1150.157767	13.464359
16.522309	1152.373617	13.469376
16.221699	1154.341098	13.474394
16.391156	1145.048810	13.479411
16.087176	1157.224006	13.484429
16.264969	1157.296576	13.489447
16.603079	1149.714492	13.494464
16.551450	1149.943946	13.499482
16.550034	1143.901112	13.504499
16.169340	1128.864691	13.509517
16.082630	1136.343811	13.514535
16.275599	1142.430602	13.519552
16.107307	1142.188839	13.524570
16.225259	1140.170205	13.529587
16.219133	1149.233967	13.534605
16.243924	1153.848265	13.539623
16.156976	1147.981399	13.544640
16.084025	1143.540518	13.549658
16.113098	1139.117388	13.554675
15.875242	1159.165241	13.559693
16.130868	1159.890649	13.564711
16.329210	1157.517373	13.569728
16.318695	1174.186758	13.574746
16.456477	1176.549349	13.579763
16.288486	1176.169745	13.584781
16.309673	1181.146055	13.589799
16.434044	1173.863519	13.594816
16.635378	1181.622118	13.599834
16.579562	1177.993326	13.604851
16.488868	1182.903520	13.609869
16.500851	1171.541292	13.614887
16.867260	1180.691803	13.619904
16.281584	1185.518221	13.624922
16.536361	1186.254794	13.629939
16.459973	1183.195139	13.634957
16.247595	1186.954260	13.639975
16.548376	1184.928572	13.644992
16.425894	1199.749258	13.650010
16.561638	1206.793161	13.655027
16.983467	1207.522545	13.660045
17.142673	1215.357426	13.665063
17.243440	1199.532173	13.670080
17.518723	1184.820524	13.675098
17.068879	1177.328357	13.680115
17.137546	1169.974340	13.685133
16.953334	1177.277112	13.690151
17.296080	1166.816779	13.695168
16.885712	1173.148368	13.700186
17.147706	1176.339971	13.705203
17.245273	1171.418890	13.710221
17.126752	1164.937974	13.715239
17.261824	1143.992688	13.720256
17.013072	1134.645647	13.725274
17.087963	1137.943419	13.730291
17.265379	1136.038163	13.735309
16.887235	1135.942565	13.740327
17.165872	1124.756286	13.745344
16.759295	1138.413369	13.750362
17.045689	1136.511719	13.755379
17.059899	1131.020615	13.760397
16.873553	1136.774560	13.765415
16.788496	1131.549098	13.770432
17.233085	1148.795829	13.775450
17.199017	1159.074028	13.780467
17.216073	1150.227432	13.785485
16.975324	1161.268181	13.790503
17.159974	1163.385221	13.795520
16.969690	1171.280710	13.800538
17.072297	1171.155106	13.805555
17.101296	1176.089177	13.810573
17.340028	1167.986549	13.815591
17.396092	1162.832981	13.820608
17.208300	1173.646472	13.825626
17.202308	1161.149861	13.830643
17.355741	1169.443928	13.835661
17.318790	1166.878518	13.840679
17.315976	1163.910223	13.845696
17.157177	1176.378313	13.850714
17.107726	1174.901553	13.855731
17.375499	1171.249886	13.860749
17.279657	1172.481907	13.865767
17.364758	1164.773607	13.870784
17.254727	1174.116787	13.875802
17.233151	1168.337510	13.880819
17.610971	1164.663684	13.885837
17.040185	1167.008967	13.890855
17.343259	1162.785332	13.895872
17.426252	1167.833290	13.900890
17.209813	1173.279643	13.905907
17.381301	1175.895700	13.910925
17.369158	1193.438184	13.915943
17.606986	1190.530820	13.920960
17.602944	1191.017741	13.925978
17.461601	1201.262946	13.930995
17.706245	1187.392171	13.936013
17.828286	1199.260640	13.941031
18.088415	1190.935565	13.946048
17.733732	1195.772946	13.951066
17.717820	1200.538877	13.956083
17.515740	1195.384345	13.961101
17.355773	1192.090504	13.966119
17.871569	1186.880090	13.971136
17.744725	1190.458123	13.976154
17.509762	1191.456498	13.981171
18.160941	1191.188875	13.986189
17.580833	1185.341456	13.991207
17.870119	1189.579299	13.996224
17.997516	1193.014447	14.001242
17.945902	1190.669565	14.006259
18.131347	1187.440570	14.011277
17.967228	1185.017078	14.016295
17.875538	1186.652732	14.021312
17.903843	1185.625680	14.026330
17.875725	1193.263624	14.031347
18.105461	1175.841887	14.036365
18.167922	1183.628995	14.041383
18.026416	1189.339314	14.046400
17.831263	1189.310261	14.051418
17.787733	1192.567421	14.056435
18.106494	1184.342479	14.061453
18.002584	1183.773135	14.066471
18.225001	1179.990792	14.071488
18.159808	1190.570220	14.076506
17.381811	1187.144871	14.081523
17.949269	1182.712494	14.086541
17.778749	1190.945260	14.091559
17.686533	1187.639807	14.096576
17.860909	1201.181059	14.101594
17.938812	1219.678319	14.106611
18.108647	1218.425078	14.111629
18.090203	1226.388199	14.116647
18.128897	1221.094972	14.121664
17.997867	1220.177371	14.126682
18.074693	1225.962569	14.131699
18.215249	1215.517182	14.136717
18.227281	1227.033821	14.141735
18.383166	1219.820452	14.146752
18.093207	1217.439445	14.151770
18.134510	1230.188213	14.156787
18.625984	1212.424283	14.161805
18.351723	1218.134943	14.166823
18.463894	1210.533158	14.171840
18.572262	1216.024556	14.176858
18.410476	1218.034409	14.181875
18.576471	1214.311399	14.186893
18.301949	1224.880240	14.191911
18.545398	1217.282696	14.196928
18.548481	1214.942926	14.201946
18.327010	1219.724004	14.206963
18.806876	1230.386424	14.211981
18.732517	1227.439020	14.216999
18.795721	1218.162708	14.222016
18.824675	1228.583662	14.227034
18.020059	1223.726924	14.232051
18.530713	1220.572413	14.237069
18.915816	1239.977069	14.242087
19.363611	1240.262009	14.247104
18.985930	1227.344229	14.252122
18.763473	1218.634892	14.257139
18.706157	1218.235778	14.262157
18.526414	1222.588306	14.267175
18.494080	1215.895069	14.272192
18.649357	1217.254404	14.277210
18.352835	1219.716872	14.282227
18.993203	1230.097209	14.287245
18.814696	1250.428257	14.292263
18.991152	1240.418629	14.297280
19.122602	1241.221296	14.302298
18.985364	1236.957959	14.307315
19.042127	1221.182095	14.312333
18.775218	1226.271873	14.317351
19.001530	1211.808458	14.322368
19.248565	1213.442747	14.327386
18.775907	1226.803772	14.332403
18.832044	1211.021723	14.337421
18.816123	1232.057694	14.342439
19.194747	1238.008664	14.347456
19.318583	1236.003609	14.352474
18.877429	1251.040890	14.357491
19.416111	1240.807110	14.362509
19.139959	1243.962254	14.367527
19.267648	1224.642450	14.372544
19.334695	1216.237920	14.377562
19.039427	1223.491783	14.382579
19.466064	1216.944584	14.387597
19.270193	1223.739086	14.392615
19.195323	1217.101317	14.397632
19.353718	1217.563309	14.402650
19.356295	1218.221178	14.407667
19.445023	1215.538494	14.412685
19.324837	1220.820503	14.417703
19.122148	1221.049383	14.422720
19.291439	1225.084278	14.427738
18.906060	1221.599417	14.432755
19.439357	1229.087326	14.437773
19.313415	1238.948126	14.442791
19.566967	1244.415886	14.447808
19.690172	1240.179890	14.452826
19.520966	1232.391624	14.457843
19.473889	1216.477060	14.462861
19.240631	1218.076712	14.467879
19.379960	1227.024704	14.472896
19.699230	1236.838942	14.477914
19.732876	1237.920790	14.482931
19.432856	1227.828658	14.487949
19.523422	1227.779062	14.492967
19.394052	1235.820004	14.497984
19.669132	1232.897409	14.503002
19.365655	1242.069124	14.508019
19.647319	1239.052526	14.513037
19.582198	1252.709858	14.518055
19.513518	1251.357925	14.523072
19.503785	1239.747675	14.528090
19.422274	1257.197784	14.533107
19.624872	1249.976271	14.538125
19.630435	1248.342367	14.543143
19.513780	1246.363355	14.548160
19.947065	1251.102160	14.553178
19.481833	1255.122454	14.558195
19.861299	1244.817795	14.563213
19.390016	1241.748719	14.568231
19.240064	1250.371802	14.573248
20.320620	1265.459466	14.578266
19.820799	1279.806112	14.583283
19.852261	1277.502577	14.588301
20.171556	1278.674130	14.593319
20.063138	1277.602785	14.598336
20.303465	1265.495212	14.603354
19.810573	1251.811469	14.608371
20.000710	1242.113347	14.613389
20.083473	1243.048875	14.618407
20.168351	1257.357339	14.623424
20.122710	1241.816517	14.628442
19.961615	1242.458578	14.633459
20.315727	1251.763526	14.638477
20.240015	1236.839091	14.643495
19.974750	1240.071956	14.648512
19.898297	1245.396730	14.653530
19.985828	1262.378707	14.658547
20.312042	1258.168536	14.663565
20.083072	1264.107141	14.668583
20.621434	1270.302531	14.673600
20.349143	1260.909313	14.678618
20.535910	1265.562569	14.683635
20.490063	1260.536078	14.688653
20.508189	1244.329985	14.693671
20.273811	1237.422172	14.698688
20.327675	1227.953311	14.703706
20.195791	1237.890289	14.708723
20.505595	1247.387213	14.713741
20.415664	1262.931685	14.718759
20.414945	1274.322521	14.723776
20.792245	1270.808989	14.728794
20.473219	1245.201081	14.733811
20.586118	1231.080043	14.738829
20.789303	1225.521393	14.743847
20.432699	1226.247401	14.748864
20.702503	1223.670554	14.753882
20.567180	1229.254277	14.758899
20.243739	1227.232347	14.763917
20.877945	1231.339859	14.768935
20.538684	1241.172994	14.773952
20.734464	1232.170382	14.778970
20.523263	1229.354295	14.783987
20.623452	1247.879001	14.789005
20.683730	1252.281158	14.794023
20.805877	1261.123356	14.799040
20.949988	1253.264693	14.804058
20.646220	1259.368434	14.809075
20.884095	1260.859366	14.814093
20.915514	1262.446690	14.819111
20.708114	1250.046743	14.824128
20.903706	1241.011087	14.829146
21.040429	1249.445363	14.834163
20.867494	1235.192523	14.839181
20.739811	1233.662572	14.844199
20.434532	1252.892992	14.849216
20.692743	1257.362372	14.854234
20.705507	1251.830128	14.859251
20.905046	1260.403216	14.864269
20.674943	1262.956658	14.869287
20.758471	1266.559320	14.874304
21.084061	1264.571639	14.879322
20.796961	1260.401613	14.884339
20.820566	1256.614773	14.889357
20.786701	1261.484480	14.894375
20.791050	1293.568091	14.899392
20.920435	1288.256280	14.904410
20.709958	1296.457137	14.909427
20.997286	1296.656842	14.914445
21.085394	1287.900763	14.919463
20.884744	1292.050083	14.924480
21.207979	1294.587490	14.929498
21.107883	1292.062042	14.934515
21.402239	1286.714646	14.939533
21.835145	1284.385971	14.944551
21.438862	1299.962313	14.949568
21.420658	1293.854879	14.954586
21.135232	1290.654625	14.959603
21.195751	1286.084517	14.964621
21.585472	1287.025122	14.969639
21.073088	1291.713454	14.974656
21.351879	1290.184297	14.979674
21.354347	1300.890388	14.984691
21.575351	1289.054494	14.989709
21.729748	1293.345411	14.994727
21.443719	1291.376331	14.999744
21.905473	1284.866596	15.004762
21.397142	1288.831438	15.009779
21.262652	1292.832798	15.014797
21.569866	1298.925141	15.019815
21.462748	1314.688648	15.024832
21.733466	1312.004157	15.029850
22.070542	1318.118334	15.034867
21.559133	1312.400038	15.039885
21.891135	1302.294930	15.044903
21.637206	1305.561757	15.049920
21.860172	1309.561409	15.054938
21.602021	1306.475136	15.059955
21.631306	1307.151420	15.064973
21.949482	1303.648459	15.069991
21.860362	1316.688575	15.075008
21.999058	1315.442057	15.080026
22.018444	1321.553332	15.085043
21.833711	1317.842314	15.090061
21.909394	1310.061488	15.095079
21.746395	1318.367090	15.100096
21.769389	1316.462187	15.105114
22.203037	1314.604635	15.110131
22.060067	1312.007151	15.115149
22.100187	1310.293897	15.120167
22.011421	1316.103007	15.125184
21.884394	1313.259187	15.130202
21.907635	1313.529788	15.135219
22.063105	1313.963528	15.140237
22.153744	1313.805655	15.145255
22.047260	1315.857543	15.150272
22.272854	1316.832809	15.155290
21.884827	1316.392789	15.160307
21.962517	1315.134721	15.165325
22.209756	1311.366345	15.170343
22.061831	1320.741871	15.175360
22.012419	1314.419916	15.180378
21.788123	1317.098387	15.185395
22.098410	1326.187808	15.190413
22.252679	1321.109656	15.195431
22.022996	1343.744529	15.200448
22.510563	1338.291106	15.205466
22.753062	1336.288042	15.210483
22.499967	1335.739459	15.215501
22.651033	1336.471168	15.220519
22.259970	1334.573805	15.225536
22.357876	1331.692341	15.230554
22.521130	1333.403114	15.235571
22.295948	1339.016716	15.240589
22.316473	1335.115408	15.245607
22.581235	1335.718843	15.250624
22.616800	1327.198996	15.255642
22.633991	1334.087002	15.260659
22.783711	1339.090503	15.265677
22.415937	1331.551993	15.270695
22.819521	1329.981302	15.275712
22.700279	1327.454294	15.280730
22.578612	1330.196086	15.285747
22.432768	1335.142231	15.290765
22.761724	1329.652873	15.295783
22.759091	1335.017028	15.300800
22.561045	1328.523621	15.305818
22.772206	1328.736333	15.310835
22.293914	1340.418107	15.315853
22.559178	1344.724930	15.320871
22.637417	1366.224221	15.325888
22.753333	1366.339715	15.330906
23.133938	1354.959224	15.335923
22.754599	1365.260876	15.340941
23.237979	1357.548339	15.345959
23.120867	1357.212666	15.350976
23.126112	1359.249208	15.355994
23.476937	1357.286076	15.361011
23.334989	1351.864846	15.366029
23.417888	1351.322828	15.371047
22.925438	1352.575658	15.376064
23.017866	1357.995337	15.381082
23.203110	1353.165584	15.386099
23.410614	1351.587597	15.391117
23.619368	1352.897931	15.396135
23.251474	1335.974577	15.401152
23.232338	1323.947325	15.406170
22.905336	1323.805461	15.411187
23.196694	1343.725368	15.416205
23.599432	1347.903130	15.421223
23.121838	1352.147932	15.426240
23.543951	1362.353087	15.431258
23.527318	1349.719899	15.436275
23.250506	1355.778270	15.441293
23.660486	1351.214447	15.446311
23.608805	1352.474995	15.451328
23.344498	1351.379066	15.456346
23.226021	1345.142944	15.461363
23.084493	1357.573673	15.466381
23.163052	1348.942367	15.471399
23.526555	1346.579113	15.476416
23.146121	1357.264005	15.481434
22.948036	1357.522832	15.486451
23.239251	1360.446648	15.491469
23.505322	1369.907583	15.496487
23.680081	1383.834357	15.501504
23.854599	1378.681574	15.506522
23.878849	1382.523603	15.511539
23.690324	1379.454525	15.516557
24.158156	1373.627594	15.521575
23.745690	1363.667771	15.526592
23.761409	1360.353069	15.531610
23.919193	1354.414891	15.536627
23.894100	1369.263312	15.541645
24.089168	1368.359418	15.546663
23.961137	1356.196238	15.551680
23.724393	1349.359631	15.556698
23.845217	1343.953158	15.561715
24.036577	1366.517161	15.566733
23.867993	1371.487950	15.571751
24.068197	1364.713624	15.576768
24.111376	1375.579951	15.581786
24.060414	1377.663203	15.586803
23.827174	1379.225075	15.591821
23.910096	1377.053945	15.596839
23.815472	1372.611076	15.601856
23.719987	1377.122525	15.606874
23.992420	1365.789072	15.611891
23.759499	1378.024720	15.616909
24.062765	1362.690956	15.621927
23.921122	1372.426096	15.626944
24.340831	1391.696081	15.631962
24.577848	1398.322127	15.636979
24.635336	1378.581480	15.641997
24.628127	1368.246284	15.647015
24.552494	1374.876455	15.652032
24.636285	1366.287579	15.657050
24.587277	1367.960277	15.662067
24.425615	1366.586331	15.667085
24.831564	1364.308957	15.672103
24.746824	1355.726735	15.677120
24.524353	1365.518168	15.682138
24.550363	1357.130200	15.687155
24.539577	1362.097690	15.692173
24.558832	1362.351629	15.697191
24.768753	1355.200901	15.702208
24.519474	1368.310888	15.707226
24.583998	1361.500764	15.712243
24.719258	1364.188599	15.717261
24.829537	1358.821268	15.722279
24.958162	1360.722420	15.727296
24.814193	1371.750835	15.732314
25.007527	1352.753460	15.737331
24.945164	1364.141971	15.742349
24.700227	1364.934926	15.747367
24.797440	1368.845576	15.752384
24.805358	1367.467957	15.757402
24.744876	1362.618262	15.762419
24.705397	1366.748787	15.767437
24.819938	1363.849996	15.772455
24.703462	1364.462232	15.777472
24.632590	1364.514958	15.782490
24.985131	1355.494584	15.787507
24.680223	1374.152268	15.792525
24.746051	1366.003761	15.797543
25.135042	1378.263982	15.802560
24.930954	1391.440912	15.807578
25.195776	1396.103723	15.812595
25.234907	1397.165777	15.817613
25.124845	1397.941122	15.822631
25.255537	1400.217916	15.827648
25.037473	1403.966612	15.832666
25.142855	1395.819020	15.837683
25.082939	1399.036811	15.842701
25.283711	1396.504831	15.847719
25.815691	1395.499870	15.852736
25.172607	1398.641003	15.857754
25.517702	1395.165454	15.862771
25.508820	1398.841716	15.867789
25.376603	1398.756177	15.872807
25.532475	1397.630035	15.877824
25.372691	1391.177116	15.882842
25.454107	1390.014092	15.887859
25.308832	1392.818858	15.892877
25.487015	1398.372381	15.897895
25.557374	1400.572946	15.902912
25.549361	1395.599987	15.907930
25.360068	1387.953943	15.912947
25.279643	1394.829400	15.917965
25.441858	1394.611249	15.922983
25.457926	1393.956676	15.928000
25.527009	1398.409779	15.933018
25.420537	1391.195287	15.938035
25.456769	1404.937149	15.943053
25.555546	1414.447073	15.948071
25.617592	1419.998969	15.953088
25.424613	1419.849871	15.958106
25.702225	1421.075582	15.963123
25.711330	1421.726079	15.968141
25.694995	1420.116648	15.973159
25.727062	1415.304367	15.978176
25.867596	1424.346759	15.983194
25.888087	1413.802619	15.988211
25.642760	1430.804860	15.993229
25.874935	1436.481343	15.998247
26.296273	1443.727272	16.003264
26.027840	1454.934228	16.008282
26.316173	1440.554424	16.013299
26.555417	1431.376785	16.018317
26.252575	1419.165339	16.023335
26.374073	1402.221502	16.028352
26.087179	1413.665340	16.033370
26.329097	1407.448646	16.038387
26.453569	1409.587497	16.043405
26.310272	1409.075059	16.048423
26.350257	1407.247645	16.053440
26.525781	1405.675342	16.058458
26.200159	1406.621814	16.063475
26.397685	1409.328086	16.068493
26.400264	1412.852456	16.073511
26.542716	1402.094823	16.078528
26.289140	1419.481876	16.083546
26.357484	1412.940779	16.088563
26.313069	1400.003494	16.093581
26.274978	1419.881204	16.098599
26.639946	1424.234531	16.103616
26.680175	1436.383655	16.108634
26.865411	1436.992389	16.113651
26.687660	1424.606683	16.118669
26.620123	1406.216212	16.123687
27.063069	1402.721702	16.128704
26.583542	1403.186975	16.133722
26.585668	1404.528380	16.138739
26.684138	1407.810889	16.143757
26.867720	1419.214225	16.148775
27.085669	1423.811973	16.153792
26.505253	1417.109409	16.158810
26.873740	1419.638163	16.163827
27.057469	1434.005617	16.168845
27.019698	1427.577753	16.173863
27.029094	1419.180298	16.178880
26.845274	1427.785859	16.183898
26.985653	1423.037922	16.188915
26.841511	1418.704418	16.193933
26.771507	1444.537754	16.198951
27.098142	1443.854192	16.203968
27.043739	1447.004939	16.208986
27.201534	1437.867161	16.214003
27.110592	1434.216960	16.219021
27.100862	1439.496107	16.224039
27.336244	1432.984426	16.229056
27.435338	1438.190435	16.234074
26.987807	1435.442972	16.239091
27.362851	1428.037705	16.244109
27.377611	1436.697395	16.249127
26.879081	1429.612373	16.254144
26.902049	1429.978296	16.259162
26.948233	1434.061190	16.264179
27.085551	1429.170059	16.269197
26.948337	1435.380538	16.274215
27.373509	1448.297019	16.279232
27.266548	1464.137422	16.284250
27.395523	1463.599188	16.289267
27.669721	1463.307769	16.294285
27.494023	1475.224965	16.299303
27.795016	1454.101000	16.304320
27.735408	1459.080936	16.309338
27.770047	1457.703608	16.314355
27.713817	1461.073556	16.319373
27.703497	1454.814361	16.324391
27.768291	1460.665419	16.329408
27.760682	1453.487283	16.334426
27.706033	1456.692403	16.339443
28.062836	1447.599223	16.344461
27.759935	1454.920598	16.349479
28.242915	1452.617465	16.354496
28.002631	1450.816771	16.359514
27.999202	1458.024778	16.364531
28.155109	1453.980157	16.369549
28.245652	1450.784934	16.374567
28.123906	1426.543252	16.379584
27.960130	1423.903919	16.384602
27.782724	1425.658121	16.389619
27.975382	1429.048658	16.394637
28.014806	1451.982036	16.399655
27.847225	1443.311515	16.404672
27.978644	1454.373914	16.409690
27.846742	1451.258438	16.414707
27.883686	1460.734536	16.419725
27.747398	1451.513166	16.424743
28.357926	1455.835288	16.429760
28.267574	1453.522765	16.434778
28.183872	1451.972123	16.439795
28.159804	1454.111168	16.444813
27.894261	1462.527921	16.449831
28.321322	1475.137029	16.454848
28.280931	1480.011428	16.459866
28.311477	1491.211815	16.464883
28.393182	1482.598417	16.469901
28.162895	1487.009781	16.474919
28.624336	1484.827138	16.479936
28.696559	1485.799072	16.484954
28.704725	1485.322574	16.489971
28.583880	1478.523016	16.494989
28.380196	1484.068150	16.500007
28.891860	1486.126754	16.505024
28.912816	1484.759564	16.510042
28.764889	1484.565604	16.515059
29.114267	1471.742969	16.520077
28.857960	1483.697142	16.525095
28.995747	1480.967707	16.530112
28.901052	1485.234571	16.535130
28.828401	1481.604952	16.540147
29.076831	1470.946650	16.545165
29.154942	1489.457978	16.550183
28.937151	1480.990237	16.555200
28.925602	1481.055974	16.560218
28.805305	1480.439726	16.565235
28.891057	1488.011322	16.570253
28.320290	1481.023670	16.575271
28.903624	1483.516858	16.580288
29.089133	1484.032243	16.585306
29.114512	1474.052206	16.590323
29.362538	1471.021450	16.595341
29.176089	1490.618703	16.600359
29.012928	1479.075411	16.605376
29.100727	1482.908516	16.610394
28.946602	1491.146600	16.615411
29.509249	1482.906314	16.620429
29.239108	1505.938670	16.625447
29.127049	1507.504109	16.630464
29.085583	1506.355125	16.635482
29.503621	1512.875655	16.640499
29.849229	1510.549987	16.645517
29.486704	1512.566740	16.650535
29.525675	1510.364682	16.655552
29.604891	1508.393359	16.660570
29.797913	1509.642533	16.665587
29.647110	1505.834119	16.670605
29.456903	1507.534545	16.675623
29.715064	1506.363111	16.680640
29.796872	1507.476766	16.685658
29.479258	1509.032149	16.690675
29.970356	1501.768259	16.695693
29.753454	1499.923137	16.700711
30.042455	1491.872646	16.705728
30.120162	1502.707754	16.710746
29.868988	1505.289134	16.715763
30.012586	1503.956751	16.720781
29.871550	1500.014833	16.725799
29.820678	1501.639429	16.730816
30.021647	1492.442896	16.735834
29.809382	1500.784706	16.740851
30.148922	1500.958840	16.745869
30.090591	1504.323240	16.750887
29.910351	1502.716926	16.755904
30.267178	1495.826057	16.760922
29.915235	1507.631520	16.765939
30.288367	1501.221015	16.770957
30.200252	1501.254943	16.775975
30.079463	1502.340336	16.780992
30.093520	1502.819545	16.786010
29.886360	1505.978277	16.791027
30.189894	1486.428243	16.796045
30.225639	1489.751864	16.801063
30.235330	1493.020746	16.806080
30.320368	1491.792155	16.811098
29.862655	1505.417476	16.816115
30.624762	1514.716834	16.821133
30.402512	1531.811033	16.826151
30.510493	1521.323984	16.831168
30.778035	1525.067100	16.836186
30.554590	1536.640284	16.841203
31.041891	1528.121114	16.846221
31.055868	1517.565383	16.851239
30.357205	1505.741851	16.856256
30.561051	1503.981385	16.861274
30.535152	1524.195003	16.866291
30.860848	1528.132425	16.871309
30.331003	1521.615140	16.876327
30.563600	1523.155004	16.881344
31.093278	1518.331156	16.886362
30.905517	1524.931534	16.891379
31.162884	1511.256787	16.896397
30.766450	1520.973582	16.901415
30.714611	1522.470390	16.906432
31.080271	1515.588286	16.911450
31.155533	1518.014826	16.916467
30.956171	1512.862887	16.921485
31.109053	1525.837514	16.926503
30.810848	1520.933435	16.931520
30.982697	1515.371603	16.936538
30.995859	1524.222156	16.941555
30.946553	1504.984067	16.946573
31.023069	1519.218568	16.951591
31.047420	1505.695796	16.956608
31.126722	1524.315629	16.961626
30.816478	1544.666515	16.966643
30.881323	1546.618803	16.971661
31.391859	1540.833164	16.976679
31.170565	1541.493472	16.981696
31.345524	1540.146838	16.986714
31.214077	1550.364650	16.991731
31.546112	1541.830238	16.996749
31.482689	1544.939586	17.001767
31.595539	1545.566216	17.006784
31.533216	1546.368703	17.011802
31.396382	1547.853603	17.016819
31.568875	1558.849826	17.021837
31.945512	1567.219745	17.026855
31.866898	1581.548101	17.031872
32.037658	1561.060908	17.036890
31.386501	1554.718814	17.041907
32.203672	1552.965049	17.046925
32.138181	1553.468457	17.051943
32.069181	1536.016258	17.056960
32.194919	1536.243512	17.061978
32.192340	1542.802210	17.066995
32.136854	1534.202446	17.072013
31.929438	1540.613960	17.077031
32.261667	1532.425582	17.082048
32.439750	1529.535136	17.087066
32.213161	1536.304939	17.092083
32.316157	1537.515481	17.097101
32.520836	1538.003284	17.102119
32.282906	1530.076642	17.107136
32.591304	1529.624442	17.112154
32.484704	1542.680240	17.117171
32.509351	1526.158995	17.122189
32.524503	1519.559732	17.127207
32.277214	1518.161762	17.132224
32.268463	1497.730361	17.137242
31.850866	1519.423782	17.142259
32.162839	1522.798125	17.147277
32.181971	1530.572505	17.152295
32.221569	1529.333325	17.157312
32.632541	1522.980325	17.162330
32.503579	1535.489431	17.167347
32.317638	1536.459237	17.172365
32.444837	1527.779226	17.177383
32.500979	1530.166020	17.182400
32.491917	1528.695137	17.187418
32.516256	1555.995702	17.192435
32.716171	1557.644131	17.197453
32.721069	1563.394910	17.202471
32.222741	1568.411309	17.207488
32.811259	1564.025733	17.212506
32.383765	1565.326090	17.217523
32.581915	1569.649996	17.222541
32.595640	1563.619058	17.227559
32.445020	1571.644007	17.232576
32.759719	1573.759649	17.237594
32.805814	1589.455938	17.242611
33.036684	1586.284694	17.247629
33.237442	1585.382601	17.252647
33.296633	1592.713372	17.257664
33.158811	1582.940998	17.262682
32.958777	1580.715121	17.267699
33.193454	1583.253462	17.272717
33.609993	1585.046337	17.277735
33.215940	1585.089194	17.282752
33.138124	1574.298625	17.287770
33.321412	1583.608046	17.292787
33.160426	1580.240275	17.297805
33.452430	1575.299074	17.302823
33.064872	1592.281343	17.307840
33.266978	1587.742031	17.312858
33.527306	1595.091072	17.317875
33.246119	1580.654658	17.322893
33.515729	1596.254888	17.327911
33.570625	1614.558006	17.332928
33.598150	1614.396407	17.337946
33.816628	1619.801211	17.342963
33.795151	1613.231596	17.347981
34.103810	1613.024625	17.352999
33.825080	1612.716102	17.358016
33.677894	1610.117298	17.363034
34.072381	1613.763824	17.368051
33.486906	1617.558451	17.373069
33.905809	1611.944258	17.378087
33.666011	1616.090698	17.383104
34.118450	1608.122532	17.388122
34.230702	1607.746510	17.393139
34.066809	1609.099676	17.398157
34.158942	1599.675040	17.403175
34.085707	1611.590728	17.408192
34.294478	1598.549935	17.413210
34.472917	1609.468832	17.418227
34.045258	1605.275136	17.423245
34.422708	1605.405593	17.428263
34.275107	1609.172591	17.433280
34.554068	1608.376052	17.438298
34.248380	1609.701124	17.443315
34.331487	1606.619304	17.448333
34.556566	1602.341931	17.453351
34.348848	1604.425187	17.458368
34.603087	1601.554794	17.463386
34.168199	1599.705992	17.468403
34.193301	1605.129820	17.473421
34.596036	1600.106497	17.478439
34.418018	1602.140346	17.483456
34.731557	1590.715671	17.488474
34.494837	1597.528517	17.493491
34.459116	1604.250602	17.498509
34.875720	1598.935219	17.503527
34.508125	1601.287467	17.508544
34.755956	1608.445277	17.513562
34.936925	1613.938180	17.518579
34.584369	1623.787930	17.523597
34.837498	1621.644094	17.528615
34.657616	1645.629426	17.533632
34.840611	1633.068069	17.538650
35.094755	1624.286668	17.543667
35.164701	1626.162925	17.548685
35.206281	1627.342699	17.553703
35.001297	1631.019205	17.558720
35.163672	1631.848268	17.563738
35.074303	1625.171779	17.568755
35.313027	1633.696855	17.573773
35.298198	1628.529281	17.578791
35.267966	1634.267794	17.583808
35.235174	1630.813036	17.588826
35.613704	1622.935841	17.593843
35.471762	1636.936940	17.598861
35.808827	1615.692609	17.603879
35.448677	1628.438103	17.608896
35.309769	1618.714311	17.613914
35.706679	1619.332490	17.618931
35.660592	1628.689370	17.623949
35.516159	1624.785383	17.628967
35.382790	1624.203577	17.633984
35.772043	1630.684436	17.639002
35.547698	1624.801951	17.644019
35.993980	1627.128095	17.649037
36.004189	1615.266229	17.654055
35.897078	1625.268644	17.659072
35.443994	1624.205134	17.664090
35.767196	1623.966228	17.669107
35.404592	1623.215295	17.674125
35.817731	1619.647721	17.679143
35.801809	1626.657088	17.684160
35.590028	1618.954023	17.689178
35.648321	1629.559365	17.694195
35.602947	1649.950387	17.699213
36.311295	1644.145340	17.704231
36.065372	1654.697531	17.709248
36.092643	1654.602903	17.714266
36.243967	1637.747571	17.719283
36.426378	1655.722930	17.724301
36.602797	1654.403210	17.729319
36.452329	1652.947068	17.734336
36.153937	1645.442978	17.739354
36.398707	1650.867455	17.744371
36.523132	1647.669337	17.749389
36.624047	1646.618026	17.754407
36.417826	1649.617182	17.759424
36.465217	1648.688120	17.764442
36.581852	1641.990504	17.769459
36.712152	1650.294567	17.774477
36.980888	1641.086724	17.779495
36.562969	1642.529201	17.784512
36.748436	1646.629245	17.789530
36.757919	1636.505673	17.794547
36.581337	1636.040865	17.799565
36.872208	1644.940777	17.804583
36.871516	1643.538181	17.809600
36.912321	1639.517297	17.814618
36.979715	1639.841222	17.819635
36.596750	1640.925549	17.824653
36.663425	1638.512979	17.829671
36.725403	1646.724810	17.834688
36.834767	1661.565814	17.839706
37.038531	1665.678975	17.844723
37.092429	1663.497258	17.849741
37.281469	1656.127803	17.854759
37.167006	1662.921614	17.859776
37.484487	1658.604122	17.864794
37.295326	1663.168961	17.869811
37.211967	1660.456035	17.874829
37.468816	1654.275354	17.879847
37.381393	1661.862719	17.884864
37.472959	1655.531848	17.889882
37.502379	1652.182137	17.894899
37.468255	1665.090604	17.899917
37.558127	1649.211972	17.904935
37.572343	1660.609280	17.909952
37.051399	1664.484964	17.914970
37.317682	1657.717679	17.919987
37.232281	1659.373995	17.925005
37.466534	1670.532905	17.930023
37.587267	1680.262193	17.935040
37.178510	1689.818928	17.940058
37.589091	1691.408865	17.945075
37.349330	1696.445874	17.950093
37.404951	1687.192191	17.955111
37.939944	1695.387926	17.960128
37.993538	1711.840581	17.965146
38.277223	1714.735791	17.970163
38.335747	1715.748198	17.975181
38.101043	1692.079926	17.980199
38.055484	1690.434755	17.985216
38.082880	1696.209811	17.990234
38.378470	1699.238087	17.995251
38.196960	1705.919002	18.000269
38.351266	1714.515582	18.005287
38.402645	1714.239403	18.010304
38.441640	1706.901856	18.015322
38.878626	1699.413370	18.020339
38.111014	1683.297165	18.025357
38.289253	1688.786216	18.030375
38.559583	1692.468676	18.035392
38.394884	1701.733035	18.040410
38.755383	1697.594630	18.045427
38.702930	1699.062029	18.050445
38.893852	1699.363926	18.055463
38.786630	1695.822658	18.060480
38.599358	1705.176191	18.065498
38.967817	1690.572257	18.070515
38.962681	1701.641303	18.075533
38.814402	1692.402089	18.080551
39.005724	1693.692506	18.085568
38.626853	1700.044682	18.090586
39.107959	1694.251261	18.095603
38.940635	1696.970756	18.100621
38.956649	1694.168928	18.105639
38.880076	1703.169088	18.110656
38.981752	1685.665229	18.115674
39.211250	1690.642249	18.120691
39.057713	1698.933889	18.125709
39.281037	1690.312279	18.130727
39.133677	1690.519010	18.135744
38.901498	1698.093355	18.140762
39.041401	1688.663116	18.145779
39.146572	1694.555215	18.150797
39.297369	1712.932727	18.155815
39.568507	1721.132797	18.160832
39.533348	1721.900874	18.165850
39.397939	1724.722963	18.170867
39.425542	1722.851499	18.175885
39.574861	1724.979193	18.180903
39.664507	1724.427383	18.185920
39.713763	1728.642918	18.190938
39.519592	1720.711294	18.195955
40.061268	1724.849226	18.200973
39.577895	1724.709233	18.205991
39.772274	1722.962909	18.211008
39.627542	1722.057783	18.216026
39.909833	1723.879992	18.221043
39.693186	1725.454503	18.226061
39.990818	1721.248943	18.231079
39.929062	1721.825753	18.236096
39.997803	1727.125862	18.241114
39.997457	1713.403454	18.246131
40.097389	1716.395628	18.251149
40.057896	1735.207828	18.256167
40.667740	1745.417192	18.261184
40.582390	1738.703375	18.266202
40.411298	1723.856074	18.271219
40.024032	1723.794656	18.276237
40.414997	1719.090174	18.281255
40.383544	1715.199740	18.286272
40.434399	1719.862648	18.291290
40.445140	1735.570058	18.296307
40.416399	1741.278048	18.301325
40.583330	1756.572606	18.306343
40.650074	1742.262287	18.311360
40.557682	1755.145044	18.316378
41.112369	1745.313801	18.321395
41.200764	1743.790145	18.326413
40.537069	1717.816082	18.331431
41.171529	1728.030414	18.336448
40.695127	1719.874263	18.341466
40.752057	1716.607386	18.346483
40.889488	1737.704477	18.351501
40.942516	1739.713471	18.356519
41.417605	1737.626567	18.361536
41.286429	1735.309343	18.366554
41.392790	1729.198040	18.371571
40.988301	1720.478010	18.376589
40.690513	1717.147821	18.381607
41.149013	1718.197935	18.386624
41.075401	1730.999609	18.391642
41.310284	1729.097758	18.396659
41.303127	1721.870603	18.401677
41.022480	1728.912434	18.406695
41.481666	1729.241958	18.411712
40.965600	1734.316070	18.416730
41.341184	1731.560207	18.421747
41.467382	1732.694481	18.426765
41.073818	1749.503505	18.431783
41.584937	1749.576397	18.436800
41.940180	1759.469660	18.441818
41.563495	1770.787682	18.446835
41.893419	1763.570046	18.451853
41.235417	1766.584978	18.456871
41.462353	1765.247435	18.461888
41.804018	1771.482689	18.466906
41.659800	1760.549835	18.471923
41.634836	1765.955632	18.476941
41.752439	1759.709777	18.481959
42.031652	1774.171580	18.486976
41.852337	1788.999090	18.491994
41.981493	1793.304563	18.497011
42.121559	1799.570454	18.502029
42.314691	1796.847941	18.507047
42.656340	1787.169667	18.512064
42.258437	1791.420286	18.517082
42.612616	1787.944329	18.522099
42.451672	1786.411955	18.527117
42.150529	1791.030021	18.532135
42.556553	1778.500513	18.537152
42.370023	1781.304306	18.542170
42.345079	1786.678217	18.547187
42.880397	1781.017128	18.552205
42.821767	1788.334430	18.557223
42.653478	1770.511790	18.562240
42.287248	1780.652881	18.567258
42.692740	1773.393593	18.572275
42.800269	1775.399867	18.577293
42.355879	1782.176314	18.582311
42.813103	1778.471482	18.587328
42.483432	1769.244936	18.592346
42.663102	1774.168028	18.597363
42.851693	1780.558555	18.602381
42.704989	1800.490566	18.607399
43.004359	1812.151400	18.612416
42.793804	1809.271713	18.617434
43.075176	1814.726802	18.622451
43.091012	1806.454844	18.627469
42.680428	1812.382390	18.632487
43.233306	1808.491238	18.637504
43.091023	1811.202668	18.642522
43.151609	1814.513979	18.647539
43.599536	1814.058746	18.652557
43.246522	1821.069295	18.657575
43.302826	1823.215160	18.662592
43.213864	1833.449352	18.667610
43.614358	1835.679566	18.672627
43.866693	1837.310684	18.677645
43.436143	1832.996535	18.682663
43.814470	1832.468969	18.687680
44.071378	1831.316224	18.692698
43.942363	1831.458107	18.697715
43.904463	1831.595532	18.702733
43.857130	1836.142055	18.707751
43.996094	1827.502449	18.712768
43.993293	1825.151749	18.717786
43.916325	1831.559105	18.722803
44.002787	1826.909345	18.727821
44.011567	1829.966241	18.732839
44.190146	1825.067367	18.737856
43.902740	1823.531914	18.742874
43.774915	1832.393390	18.747891
44.169743	1823.124403	18.752909
44.023970	1834.629828	18.757927
43.974266	1834.480622	18.762944
44.224262	1842.842922	18.767962
44.418255	1863.368212	18.772979
44.623873	1857.992796	18.777997
44.548349	1861.574689	18.783015
44.562365	1860.204678	18.788032
44.697388	1857.856743	18.793050
44.613535	1853.972195	18.798067
44.881136	1847.140436	18.803085
44.624350	1858.509141	18.808103
44.690859	1848.702764	18.813120
44.952138	1847.942607	18.818138
45.042682	1853.685611	18.823155
45.276508	1843.510582	18.828173
44.979391	1847.441374	18.833191
45.315468	1841.749082	18.838208
45.181495	1847.171383	18.843226
44.908799	1852.358779	18.848243
45.209329	1846.964894	18.853261
45.318991	1839.364399	18.858279
45.339437	1842.918192	18.863296
45.251805	1844.441036	18.868314
45.169102	1844.870530	18.873331
45.488677	1839.634914	18.878349
44.985227	1845.978642	18.883367
45.126892	1843.768587	18.888384
45.168014	1841.819278	18.893402
45.060475	1841.303266	18.898419
45.714508	1856.003872	18.903437
45.324301	1871.536469	18.908455
45.597373	1873.633850	18.913472
45.924002	1878.752329	18.918490
45.396831	1879.589285	18.923507
45.640014	1870.859562	18.928525
45.758002	1883.164274	18.933543
45.471287	1871.969499	18.938560
45.775258	1874.115700	18.943578
45.597479	1881.190173	18.948595
46.030336	1866.914000	18.953613
46.175621	1875.798781	18.958631
46.152871	1857.444847	18.963648
46.003306	1860.664586	18.968666
45.847234	1873.107585	18.973683
46.209172	1882.434062	18.978701
46.468913	1897.079129	18.983719
46.406175	1897.547051	18.988736
46.384803	1897.509690	18.993754
46.477230	1898.170427	18.998771
46.925835	1895.745363	19.003789
46.609251	1897.602191	19.008807
46.692839	1884.237000	19.013824
46.738639	1873.287169	19.018842
46.816976	1858.950019	19.023859
46.876138	1850.073217	19.028877
46.672494	1855.205872	19.033895
46.647327	1856.136870	19.038912
46.729307	1862.741938	19.043930
46.580070	1883.637874	19.048947
46.987920	1884.617252	19.053965
47.295397	1886.876656	19.058983
46.980412	1893.006516	19.064000
47.305952	1889.895521	19.069018
46.986968	1885.505008	19.074035
46.996722	1881.667552	19.079053
47.146658	1886.376703	19.084071
47.183563	1876.470091	19.089088
47.132448	1882.600742	19.094106
46.933059	1885.749601	19.099123
47.007412	1877.449017	19.104141
47.169106	1882.197165	19.109159
47.612574	1902.224104	19.114176
47.863392	1895.639989	19.119194
47.566532	1908.421295	19.124211
47.498147	1901.183722	19.129229
47.728624	1911.072152	19.134247
47.570802	1904.165928	19.139264
47.845348	1904.990606	19.144282
47.606559	1911.722040	19.149299
48.001506	1905.155395	19.154317
48.028903	1908.061977	19.159335
47.907057	1900.207262	19.164352
47.837327	1904.254356	19.169370
47.805113	1908.847216	19.174387
48.156085	1902.276436	19.179405
48.164472	1905.292467	19.184423
48.245744	1901.174261	19.189440
48.256639	1899.433498	19.194458
47.854724	1907.191957	19.199475
48.067160	1906.476500	19.204493
48.070732	1906.266108	19.209511
48.013662	1928.433085	19.214528
48.470415	1936.624189	19.219546
48.266789	1938.219006	19.224563
48.585127	1932.315835	19.229581
48.756082	1932.598209	19.234599
48.421502	1936.849405	19.239616
48.920925	1931.083575	19.244634
48.702453	1941.782598	19.249651
48.834625	1936.424435	19.254669
48.573916	1938.426350	19.259687
48.287814	1935.542218	19.264704
48.352372	1940.808447	19.269722
48.468952	1940.582885	19.274739
48.901341	1947.431941	19.279757
48.934486	1953.425043	19.284775
48.846480	1953.279816	19.289792
48.908376	1952.057777	19.294810
48.622429	1955.634377	19.299827
49.213877	1970.487978	19.304845
49.417727	1980.233613	19.309863
49.173894	1988.547445	19.314880
49.657736	1979.610879	19.319898
49.809086	1980.586672	19.324915
49.892230	1974.590931	19.329933
50.120581	1959.967819	19.334951
49.696144	1949.555651	19.339968
49.934887	1935.767078	19.344986
49.820843	1949.566197	19.350003
49.858073	1935.661776	19.355021
50.007678	1943.106878	19.360039
49.902493	1943.801914	19.365056
50.103531	1930.708972	19.370074
49.826407	1941.637790	19.375091
50.275384	1943.762747	19.380109
50.092433	1932.202707	19.385127
49.665260	1938.052337	19.390144
50.435951	1933.844374	19.395162
50.348078	1940.192950	19.400179
49.900978	1938.930389	19.405197
50.274574	1946.867153	19.410215
50.192548	1963.166544	19.415232
50.507147	1966.440550	19.420250
50.241303	1969.522082	19.425267
50.353181	1969.409112	19.430285
50.583362	1966.998946	19.435303
50.291644	1966.561853	19.440320
50.475453	1966.501934	19.445338
50.403031	1963.785175	19.450355
50.597356	1959.269486	19.455373
50.791058	1955.380292	19.460391
50.515434	1959.569763	19.465408
51.308057	1972.194734	19.470426
50.924256	1985.975166	19.475443
50.653073	1978.015216	19.480461
51.461202	1977.031428	19.485479
50.915839	1980.855718	19.490496
51.026309	1975.860985	19.495514
51.173921	1982.183971	19.500531
51.332749	1983.947914	19.505549
51.385610	1982.387992	19.510567
50.964361	1994.560424	19.515584
51.063143	1980.813885	19.520602
51.297613	1979.877054	19.525619
51.038129	1980.654729	19.530637
51.805196	1985.136916	19.535655
51.336173	1997.635772	19.540672
51.485797	2006.650228	19.545690
51.575805	2012.892999	19.550707
51.470790	2016.516032	19.555725
51.896075	2012.141617	19.560743
51.337131	2010.715282	19.565760
51.853751	2003.776078	19.570778
51.819933	2015.579641	19.575795
51.621955	2017.538894	19.580813
52.098515	2011.037826	19.585831
51.937087	2034.776603	19.590848
52.415240	2029.051662	19.595866
52.174553	2043.112785	19.600883
52.058150	2040.715508	19.605901
52.419245	2039.862827	19.610919
52.334824	2034.920426	19.615936
52.772752	2027.654076	19.620954
52.814288	2030.819371	19.625971
52.334750	2017.798104	19.630989
52.843771	2016.318947	19.636007
52.759317	2020.034249	19.641024
52.837564	2004.562700	19.646042
52.327487	2005.611010	19.651059
52.404429	2027.186632	19.656077
52.639460	2012.650556	19.661095
52.502133	2024.101572	19.666112
52.523781	2023.285415	19.671130
52.671366	2034.434530	19.676147
52.599128	2030.162177	19.681165
53.130074	2041.376562	19.686183
52.769001	2052.278806	19.691200
53.271743	2052.661759	19.696218
53.285806	2057.599765	19.701235
53.267677	2061.574573	19.706253
53.308006	2049.670380	19.711271
53.384863	2054.160180	19.716288
53.588020	2057.947948	19.721306
53.487457	2050.680594	19.726323
53.830271	2045.328854	19.731341
53.821690	2047.272103	19.736359
53.487337	2049.888604	19.741376
53.735654	2054.121267	19.746394
53.919559	2049.457668	19.751411
53.402211	2058.329833	19.756429
54.171355	2047.564836	19.761447
53.636612	2046.125041	19.766464
53.694680	2047.199752	19.771482
53.790888	2054.570282	19.776499
53.586990	2073.148690	19.781517
54.296684	2074.345431	19.786535
54.070019	2072.897141	19.791552
54.470736	2071.959156	19.796570
54.115840	2070.945891	19.801587
54.193315	2077.049814	19.806605
54.590086	2069.018978	19.811623
54.159054	2068.263602	19.816640
54.445698	2067.991374	19.821658
54.595767	2076.016007	19.826675
54.451387	2073.919822	19.831693
54.619467	2071.873476	19.836711
54.750266	2082.632481	19.841728
54.983158	2089.195728	19.846746
54.624426	2087.298819	19.851763
54.484332	2101.026792	19.856781
54.916195	2094.347653	19.861799
54.976629	2097.576370	19.866816
55.272180	2103.260717	19.871834
55.058689	2097.153413	19.876851
54.974335	2095.615019	19.881869
55.319679	2093.130251	19.886887
54.919752	2097.213565	19.891904
54.971006	2091.712838	19.896922
55.133412	2099.857884	19.901939
54.881367	2106.572698	19.906957
55.429207	2116.752420	19.911975
55.144069	2119.722211	19.916992
55.273514	2126.475442	19.922010
55.681111	2118.943985	19.927027
55.515909	2126.075543	19.932045
55.588913	2111.215800	19.937063
55.372765	2119.016834	19.942080
55.864681	2127.845939	19.947098
56.006088	2138.156756	19.952115
55.839341	2149.861168	19.957133
56.240555	2140.205492	19.962151
56.390406	2153.026418	19.967168
56.450031	2130.699729	19.972186
56.387725	2116.158853	19.977203
56.242745	2116.245112	19.982221
56.567730	2103.799632	19.987239
56.229426	2107.612107	19.992256
56.174254	2104.263314	19.997274
56.392799	2111.843150	20.002291
56.474923	2132.904266	20.007309
56.639407	2135.990167	20.012327
56.613018	2136.218605	20.017344
56.596077	2138.711693	20.022362
56.732607	2139.833263	20.027379
56.810401	2136.846710	20.032397
56.964410	2140.818626	20.037415
56.765917	2134.620238	20.042432
56.382941	2141.711876	20.047450
56.889147	2134.312907	20.052467
56.572685	2137.552464	20.057485
56.974461	2150.960828	20.062503
57.375103	2168.320706	20.067520
57.090763	2158.280487	20.072538
57.396465	2164.213578	20.077555
57.149272	2163.252553	20.082573
57.350628	2155.109932	20.087591
57.342004	2159.030434	20.092608
57.850446	2154.943794	20.097626
58.034630	2161.662386	20.102643
57.513349	2154.154400	20.107661
57.769612	2158.474362	20.112679
57.659912	2156.118084	20.117696
57.582238	2159.123611	20.122714
57.554712	2146.725444	20.127731
57.336879	2159.309217	20.132749
58.101171	2174.734809	20.137767
58.100652	2179.447308	20.142784
58.132387	2179.928337	20.147802
58.426570	2180.360396	20.152819
58.279022	2177.957230	20.157837
58.441957	2178.610241	20.162855
58.400586	2186.233938	20.167872
58.185681	2182.263130	20.172890
58.545450	2180.251567	20.177907
58.408401	2183.303545	20.182925
58.698151	2177.379818	20.187943
58.555781	2169.043703	20.192960
58.715593	2169.965350	20.197978
58.973773	2165.323671	20.202995
58.581384	2170.089637	20.208013
58.813517	2176.855415	20.213031
58.976794	2179.541511	20.218048
58.603332	2176.035557	20.223066
58.995444	2175.397427	20.228083
58.785792	2183.234033	20.233101
58.863397	2190.100998	20.238119
58.921498	2202.287134	20.243136
59.037263	2205.859086	20.248154
59.149921	2196.920077	20.253171
59.147994	2204.723086	20.258189
59.127929	2196.643879	20.263207
59.529051	2206.590072	20.268224
59.653673	2209.177057	20.273242
59.606390	2200.569266	20.278259
59.835160	2218.809659	20.283277
60.062397	2208.763047	20.288295
60.009576	2205.994573	20.293312
59.894266	2197.789793	20.298330
59.999299	2187.331131	20.303347
59.663861	2200.819876	20.308365
59.574160	2191.118680	20.313383
59.794914	2214.489318	20.318400
59.824683	2226.239204	20.323418
60.359858	2213.544651	20.328435
60.186052	2216.170423	20.333453
60.330194	2220.430225	20.338471
60.301675	2223.884335	20.343488
60.086275	2228.630067	20.348506
60.269994	2219.796212	20.353523
60.061719	2222.674158	20.358541
60.462120	2243.600043	20.363559
60.847021	2240.503167	20.368576
60.835475	2246.937264	20.373594
60.895292	2247.596723	20.378611
60.835618	2253.617515	20.383629
60.789721	2246.097307	20.388647
61.013284	2251.185732	20.393664
60.754292	2252.150352	20.398682
60.810861	2237.644011	20.403699
60.628851	2248.872660	20.408717
61.041062	2250.630900	20.413735
61.197763	2265.834738	20.418752
61.069537	2277.834061	20.423770
61.548116	2280.430956	20.428787
61.325376	2286.411437	20.433805
61.262132	2283.173395	20.438823
61.781614	2277.045836	20.443840
61.702775	2283.406835	20.448858
61.932892	2271.871062	20.453875
61.683679	2276.510592	20.458893
61.745011	2274.555915	20.463911
61.968984	2264.996442	20.468928
61.841893	2258.695626	20.473946
62.209458	2267.203262	20.478963
61.978734	2263.278754	20.483981
62.185672	2262.948853	20.488999
62.320401	2261.385190	20.494016
62.578028	2264.285608	20.499034
62.442466	2253.920286	20.504051
62.507841	2257.319484	20.509069
62.202779	2259.531546	20.514087
62.480226	2257.273359	20.519104
62.580033	2259.199869	20.524122
62.398949	2255.629756	20.529139
62.764883	2270.117430	20.534157
62.999738	2283.610244	20.539175
63.035685	2289.508126	20.544192
62.748781	2290.989597	20.549210
62.937103	2290.490330	20.554227
62.724419	2294.622615	20.559245
62.983678	2287.080993	20.564263
63.000738	2280.145643	20.569280
62.888872	2294.139203	20.574298
63.234607	2277.376583	20.579315
63.210477	2284.702186	20.584333
63.148672	2282.471822	20.589351
63.293755	2281.163933	20.594368
63.183642	2288.037614	20.599386
63.531688	2303.166102	20.604403
63.425502	2316.206732	20.609421
63.458001	2309.155029	20.614439
63.714152	2312.382487	20.619456
63.665317	2312.819771	20.624474
63.891225	2310.534676	20.629491
63.628544	2310.386476	20.634509
63.495818	2314.853574	20.639527
63.943738	2308.113415	20.644544
63.653132	2320.942844	20.649562
64.159392	2325.611239	20.654579
63.917133	2331.826869	20.659597
64.118011	2341.001545	20.664615
64.208359	2325.056787	20.669632
64.157048	2336.898532	20.674650
64.416683	2328.470174	20.679667
64.692557	2325.412202	20.684685
64.462034	2335.208725	20.689703
64.376328	2334.116614	20.694720
64.719800	2348.526187	20.699738
64.728364	2358.289435	20.704755
64.902364	2358.448080	20.709773
64.444730	2359.696004	20.714791
64.832390	2358.490468	20.719808
64.936626	2361.681277	20.724826
64.943636	2352.753766	20.729843
65.054403	2354.976912	20.734861
64.941992	2361.823446	20.739879
65.268089	2355.051075	20.744896
65.447954	2370.876012	20.749914
65.172553	2385.532983	20.754931
65.631614	2376.907396	20.759949
65.525232	2386.415273	20.764967
65.824400	2369.428758	20.769984
65.602459	2384.075300	20.775002
65.588092	2379.160955	20.780019
66.009733	2374.302375	20.785037
66.105929	2384.572415	20.790055
66.161697	2372.237838	20.795072
66.106985	2377.115677	20.800090
66.196299	2375.492984	20.805107
66.129790	2372.735802	20.810125
66.287789	2373.543977	20.815143
66.172508	2372.940247	20.820160
65.958482	2369.217288	20.825178
66.075420	2364.959190	20.830195
66.323672	2394.190781	20.835213
66.499963	2410.650633	20.840231
66.484430	2404.950607	20.845248
66.791176	2405.181765	20.850266
66.687189	2407.873176	20.855283
66.736241	2404.757860	20.860301
66.919858	2402.146273	20.865319
67.403434	2399.109804	20.870336
67.349703	2404.094975	20.875354
67.511968	2401.948363	20.880371
67.292732	2391.768072	20.885389
67.539733	2390.373216	20.890407
67.533765	2391.545173	20.895424
67.350669	2400.582273	20.900442
67.243611	2383.052347	20.905459
67.270935	2390.221048	20.910477
67.177871	2392.622839	20.915495
67.440789	2395.489334	20.920512
67.130521	2396.966808	20.925530
67.520628	2408.005953	20.930547
67.854174	2415.784229	20.935565
67.810073	2425.946024	20.940583
67.920524	2418.446696	20.945600
67.808186	2422.947458	20.950618
67.997593	2425.913536	20.955635
67.714438	2415.324895	20.960653
67.785987	2423.402868	20.965671
67.717254	2421.462622	20.970688
68.173293	2441.977180	20.975706
67.867074	2438.274982	20.980723
68.189614	2445.190484	20.985741
68.097623	2447.241300	20.990759
68.412346	2442.726010	20.995776
68.395965	2466.052036	21.000794
68.388337	2471.331973	21.005811
68.734283	2474.035120	21.010829
68.681900	2476.338845	21.015847
68.842816	2469.223677	21.020864
68.831137	2476.815433	21.025882
68.759534	2470.934106	21.030899
69.315889	2471.469622	21.035917
69.209911	2477.811965	21.040935
69.390929	2471.807701	21.045952
69.082825	2494.871821	21.050970
69.468466	2488.132844	21.055987
69.889471	2496.370327	21.061005
69.503619	2497.889067	21.066023
69.837857	2481.026946	21.071040
69.949208	2485.239886	21.076058
70.125925	2484.478741	21.081075
70.194706	2491.331158	21.086093
69.859391	2483.556772	21.091111
70.055727	2469.332206	21.096128
69.462929	2477.974567	21.101146
69.566440	2487.050092	21.106163
69.869840	2482.795341	21.111181
70.030965	2474.728117	21.116199
70.247867	2473.346112	21.121216
69.985210	2498.974505	21.126234
70.311769	2509.374997	21.131251
70.562758	2503.857588	21.136269
70.444287	2516.373618	21.141287
70.582958	2508.208514	21.146304
70.284020	2517.382586	21.151322
70.216676	2509.829185	21.156339
70.987576	2520.753387	21.161357
70.587081	2539.033387	21.166375
71.326417	2539.432302	21.171392
71.280545	2535.376717	21.176410
71.000476	2543.062161	21.181427
71.232414	2532.612178	21.186445
71.245727	2538.687535	21.191463
71.342319	2536.884869	21.196480
71.431559	2528.364139	21.201498
71.295275	2532.472811	21.206515
71.609975	2532.465240	21.211533
71.635928	2539.479896	21.216551
71.565359	2552.436081	21.221568
71.921315	2555.925821	21.226586
71.895813	2565.010942	21.231603
71.911883	2555.749905	21.236621
71.994016	2557.678592	21.241639
72.357953	2557.686490	21.246656
72.205191	2557.744510	21.251674
72.211055	2562.670648	21.256691
72.498798	2548.344650	21.261709
72.220859	2561.728115	21.266727
72.460868	2550.849987	21.271744
72.449597	2557.505046	21.276762
72.571264	2553.742993	21.281779
72.545443	2552.470074	21.286797
72.390124	2557.995768	21.291815
72.455430	2550.026265	21.296832
72.701977	2572.608480	21.301850
72.610302	2584.698843	21.306867
72.928310	2582.234670	21.311885
72.477152	2584.158743	21.316903
72.918610	2591.392042	21.321920
72.992472	2581.300899	21.326938
73.036452	2590.017814	21.331955
73.098662	2610.016668	21.336973
73.259839	2613.036279	21.341991
73.762222	2611.507380	21.347008
73.691852	2618.101773	21.352026
73.496156	2618.797257	21.357043
74.022308	2609.634417	21.362061
74.016371	2605.975769	21.367079
73.857217	2605.193456	21.372096
74.063548	2607.718158	21.377114
73.932679	2605.533437	21.382131
74.117522	2603.308252	21.387149
73.963174	2603.214556	21.392167
74.279122	2588.568084	21.397184
74.647833	2588.366912	21.402202
74.360612	2600.821970	21.407219
74.590376	2589.208458	21.412237
74.482741	2595.824368	21.417255
74.431610	2589.850230	21.422272
74.492088	2608.009885	21.427290
74.398464	2619.225347	21.432307
74.864195	2615.837439	21.437325
74.971256	2622.090624	21.442343
74.784466	2631.929308	21.447360
74.900770	2627.047188	21.452378
74.758010	2630.441559	21.457395
75.108293	2627.868878	21.462413
75.090250	2638.407623	21.467431
75.362285	2646.612369	21.472448
75.446014	2659.199765	21.477466
75.522803	2653.603267	21.482483
75.620636	2652.794542	21.487501
75.513436	2661.620000	21.492519
75.511878	2655.470689	21.497536
75.569693	2650.242318	21.502554
75.785569	2652.977665	21.507571
75.835880	2651.148396	21.512589
75.690741	2662.290523	21.517607
75.938397	2682.243801	21.522624
76.285163	2677.989299	21.527642
76.121136	2677.251886	21.532659
76.300546	2675.927651	21.537677
76.394666	2683.932727	21.542695
76.324911	2680.665757	21.547712
76.897058	2681.547510	21.552730
76.737547	2676.518906	21.557747
77.052119	2670.980673	21.562765
76.927183	2675.108765	21.567783
76.991262	2671.869640	21.572800
77.264664	2665.890953	21.577818
77.292994	2672.175306	21.582835
77.492338	2657.232702	21.587853
77.186683	2672.099688	21.592871
77.172833	2662.572657	21.597888
77.160673	2670.892588	21.602906
77.328731	2669.232809	21.607923
77.293344	2663.956870	21.612941
77.571792	2670.741183	21.617959
77.688755	2680.170128	21.622976
77.853549	2683.137182	21.627994
77.680696	2687.479131	21.633011
77.737890	2682.874910	21.638029
77.674838	2686.670296	21.643047
77.796948	2682.242346	21.648064
77.759795	2677.411213	21.653082
77.898214	2680.479491	21.658099
77.807436	2680.364637	21.663117
78.000105	2696.901614	21.668135
77.851907	2716.502737	21.673152
78.214697	2716.992750	21.678170
78.119860	2724.622414	21.683187
78.127443	2716.741129	21.688205
78.591611	2732.637085	21.693223
78.583229	2742.886879	21.698240
78.707539	2744.373929	21.703258
78.834037	2752.431164	21.708275
79.011013	2727.694254	21.713293
79.058372	2730.020480	21.718311
79.108150	2736.971040	21.723328
79.283260	2735.790042	21.728346
79.161382	2739.746372	21.733363
79.328867	2728.433641	21.738381
79.358556	2735.528088	21.743399
79.063761	2755.939809	21.748416
79.806685	2748.088731	21.753434
79.802392	2761.390047	21.758451
79.856768	2754.678639	21.763469
79.789303	2757.505412	21.768487
80.024771	2766.279309	21.773504
80.364921	2753.246903	21.778522
79.945632	2751.499315	21.783539
80.317519	2749.374251	21.788557
80.593280	2749.077437	21.793575
80.464690	2754.910608	21.798592
80.512772	2755.183815	21.803610
80.430848	2756.640836	21.808627
80.340880	2744.454514	21.813645
80.311313	2744.390947	21.818663
80.505832	2765.144525	21.823680
80.784268	2770.680368	21.828698
80.925429	2778.526906	21.833715
80.834048	2772.627478	21.838733
80.686697	2766.706608	21.843751
80.833292	2778.756488	21.848768
81.108356	2776.966767	21.853786
81.165666	2794.191269	21.858803
81.197747	2803.402831	21.863821
81.397800	2804.930499	21.868839
81.776255	2798.279200	21.873856
81.574336	2791.168055	21.878874
81.976869	2791.723543	21.883891
81.736079	2788.341552	21.888909
82.104873	2789.312499	21.893927
81.972752	2798.582351	21.898944
82.189137	2787.802465	21.903962
82.313480	2795.302951	21.908979
82.194660	2782.504402	21.913997
82.350555	2781.741967	21.919015
82.279682	2783.992101	21.924032
82.149191	2777.397914	21.929050
82.578887	2805.678515	21.934067
82.568801	2813.407190	21.939085
82.627528	2817.325368	21.944103
82.673587	2812.374107	21.949120
82.519548	2815.309326	21.954138
82.534570	2819.753678	21.959155
82.849629	2814.769294	21.964173
82.844048	2820.775443	21.969191
82.971183	2839.990161	21.974208
83.317354	2845.268733	21.979226
82.853634	2848.964740	21.984243
83.091457	2852.581597	21.989261
83.159191	2846.041574	21.994279
83.079617	2847.442304	21.999296
83.788368	2858.548705	22.004314
83.426594	2868.500769	22.009331
83.722690	2870.566128	22.014349
84.076557	2879.174411	22.019367
83.661502	2871.954807	22.024384
84.221053	2866.446815	22.029402
84.421507	2860.357682	22.034419
84.161203	2858.153015	22.039437
84.581238	2859.306836	22.044455
84.049615	2860.008341	22.049472
84.440818	2860.199537	22.054490
84.312286	2860.201966	22.059507
83.831276	2882.118030	22.064525
84.446985	2888.785960	22.069543
84.571826	2897.129788	22.074560
84.327519	2890.139798	22.079578
84.579604	2908.504711	22.084595
84.845252	2919.078176	22.089613
85.340882	2922.411004	22.094631
84.956294	2924.192587	22.099648
85.535390	2920.968143	22.104666
85.477963	2917.193528	22.109683
85.291250	2917.331585	22.114701
85.846202	2910.509271	22.119719
85.438250	2923.772435	22.124736
85.556379	2927.298096	22.129754
85.861180	2941.372470	22.134771
86.008211	2942.563627	22.139789
86.194248	2937.593086	22.144807
86.291637	2939.059414	22.149824
86.460681	2941.659248	22.154842
86.608542	2943.188091	22.159859
86.467516	2940.432121	22.164877
86.569854	2935.677032	22.169895
86.491724	2947.643770	22.174912
86.700557	2942.255245	22.179930
86.874447	2934.005341	22.184947
86.562629	2943.834998	22.189965
87.178888	2926.406761	22.194983
86.701166	2932.486797	22.200000
86.975585	2926.904726	22.205018
87.059770	2932.751555	22.210035
87.328512	2938.642243	22.215053
87.121798	2947.395749	22.220071
87.285972	2960.564213	22.225088
86.975539	2958.728098	22.230106
87.034287	2965.803664	22.235123
87.129339	2966.029725	22.240141
87.710824	2973.228207	22.245159
87.385048	2988.577999	22.250176
87.475261	2994.220292	22.255194
87.862032	2986.151666	22.260211
87.826575	2989.270057	22.265229
88.158586	3000.072373	22.270247
88.174040	3012.793417	22.275264
88.202425	3013.576628	22.280282
88.463076	3016.101853	22.285299
88.150312	3014.605517	22.290317
88.638329	3012.904930	22.295335
88.648684	3012.942635	22.300352
88.632508	3010.125820	22.305370
89.078388	3001.795408	22.310387
88.770170	3002.338263	22.315405
88.737883	3011.175532	22.320423
88.919834	3023.562298	22.325440
88.913106	3031.304305	22.330458
89.319675	3034.382195	22.335475
89.097208	3045.635439	22.340493
89.632847	3031.419936	22.345511
89.573878	3038.590230	22.350528
89.283356	3035.280598	22.355546
90.131882	3036.194179	22.360563
89.610117	3034.050889	22.365581
89.616159	3035.840647	22.370599
89.641893	3059.772847	22.375616
89.816447	3052.434271	22.380634
89.975407	3049.269917	22.385651
89.806819	3052.553290	22.390669
89.937417	3066.530232	22.395687
90.304804	3079.867924	22.400704
90.007593	3083.182838	22.405722
90.306679	3074.994421	22.410739
90.378219	3087.566463	22.415757
90.814322	3102.347263	22.420775
90.735073	3109.948940	22.425792
90.980742	3106.797385	22.430810
91.411764	3108.231324	22.435827
90.997030	3106.237247	22.440845
91.173803	3102.554924	22.445863
91.198772	3109.789706	22.450880
91.316426	3105.430099	22.455898
91.488164	3106.506143	22.460915
91.507136	3122.827822	22.465933
91.796066	3123.972661	22.470951
91.702774	3135.628243	22.475968
91.815685	3133.672400	22.480986
92.288844	3131.858502	22.486003
91.905630	3131.216420	22.491021
92.356403	3128.239976	22.496039
92.282328	3126.725369	22.501056
92.168154	3123.141220	22.506074
92.734731	3125.847328	22.511091
92.315179	3127.001197	22.516109
92.476624	3134.107477	22.521127
92.675308	3148.892589	22.526144
92.895583	3152.331303	22.531162
92.894751	3146.675427	22.536179
92.819384	3147.754590	22.541197
92.898839	3134.622893	22.546215
93.071558	3140.593736	22.551232
92.923995	3154.112828	22.556250
93.632960	3163.045187	22.561267
93.853061	3171.532854	22.566285
93.691730	3176.889665	22.571303
93.595070	3172.280850	22.576320
93.518085	3169.752054	22.581338
94.035801	3165.493135	22.586355
93.940382	3172.397058	22.591373
93.991957	3170.255283	22.596391
93.886332	3175.081953	22.601408
93.713609	3175.695300	22.606426
94.385971	3188.748315	22.611443
94.125685	3198.610941	22.616461
94.360641	3199.261917	22.621479
94.467256	3202.702530	22.626496
94.221952	3204.217750	22.631514
94.951824	3192.963549	22.636531
94.429719	3207.257371	22.641549
94.584870	3216.887820	22.646567
95.014437	3227.237877	22.651584
94.833337	3228.421963	22.656602
95.132627	3224.084222	22.661619
94.945392	3225.635109	22.666637
94.969154	3241.396219	22.671655
95.371474	3243.598781	22.676672
95.332639	3254.383142	22.681690
95.723852	3253.006072	22.686707
95.722918	3254.841108	22.691725
95.622312	3244.408307	22.696743
95.869594	3246.477862	22.701760
95.786387	3253.694398	22.706778
96.242521	3258.558408	22.711795
96.202289	3266.675803	22.716813
96.379882	3278.980807	22.721831
96.512802	3274.778090	22.726848
96.524045	3277.934874	22.731866
96.623854	3261.711974	22.736883
96.767590	3268.866135	22.741901
96.991844	3261.500726	22.746919
97.156373	3258.518892	22.751936
97.059233	3261.013233	22.756954
97.104266	3251.561929	22.761971
97.000632	3260.068203	22.766989
97.336348	3283.143825	22.772007
97.158011	3287.474641	22.777024
97.581783	3295.133686	22.782042
97.490294	3289.701846	22.787059
97.507031	3297.610590	22.792077
97.387880	3291.037145	22.797095
97.417747	3303.608386	22.802112
97.611397	3317.738517	22.807130
98.057509	3315.789299	22.812147
98.079747	3324.929956	22.817165
98.380090	3318.049614	22.822183
98.430276	3327.900289	22.827200
98.505976	3330.347516	22.832218
98.475347	3333.480926	22.837235
98.537772	3348.389193	22.842253
98.576538	3345.563614	22.847271
98.927613	3344.097896	22.852288
98.813987	3345.416898	22.857306
99.316455	3334.946000	22.862323
98.939407	3341.518634	22.867341
99.224126	3359.906632	22.872359
99.591940	3362.104294	22.877376
99.405662	3375.591400	22.882394
99.576888	3358.321421	22.887411
99.651491	3378.697203	22.892429
99.666079	3375.509832	22.897447
99.914372	3369.360608	22.902464
99.855342	3375.023418	22.907482
100.082140	3361.895484	22.912499
100.092378	3372.316249	22.917517
100.240898	3381.158440	22.922535
100.520035	3393.017540	22.927552
100.277446	3391.680825	22.932570
100.725869	3391.024275	22.937587
100.495127	3398.208212	22.942605
100.719119	3392.203569	22.947623
100.762698	3391.655394	22.952640
100.467095	3403.986872	22.957658
101.145396	3415.099111	22.962675
100.879128	3426.993811	22.967693
100.951963	3420.388917	22.972711
101.224608	3424.227728	22.977728
101.172062	3427.718763	22.982746
101.219079	3435.355997	22.987763
101.398524	3445.501916	22.992781
101.190968	3444.981146	22.997799
101.443397	3443.410872	23.002816
101.627495	3462.134192	23.007834
102.183757	3465.528764	23.012851
101.804364	3475.326235	23.017869
102.009123	3480.604422	23.022887
102.231754	3475.390223	23.027904
101.763084	3474.706362	23.032922
102.407067	3485.838115	23.037939
102.651693	3494.498690	23.042957
102.389555	3506.831008	23.047975
102.823984	3503.147274	23.052992
102.810629	3502.752239	23.058010
103.174566	3495.845147	23.063027
103.177983	3493.957788	23.068045
103.292801	3488.168453	23.073063
103.633865	3494.232440	23.078080
103.365051	3516.995461	23.083098
103.409589	3510.529876	23.088115
103.931396	3511.919292	23.093133
103.729810	3509.046067	23.098151
104.432014	3502.619248	23.103168
103.867386	3516.395525	23.108186
104.340825	3516.282532	23.113203
104.197931	3511.709622	23.118221
104.484146	3512.216281	23.123239
104.728332	3507.515889	23.128256
104.746969	3509.678069	23.133274
104.594463	3502.126868	23.138291
104.740356	3502.355938	23.143309
104.919401	3508.010089	23.148327
104.779722	3503.350025	23.153344
104.790247	3513.815331	23.158362
105.007577	3516.636823	23.163379
105.025995	3530.929247	23.168397
104.329545	3533.938659	23.173415
105.282630	3540.318309	23.178432
104.927900	3563.130666	23.183450
104.985049	3567.856480	23.188467
105.283583	3577.447268	23.193485
105.535796	3598.859022	23.198503
105.866876	3594.861235	23.203520
105.720667	3598.816691	23.208538
105.857488	3609.765150	23.213555
106.093102	3618.215055	23.218573
106.246156	3616.366693	23.223591
106.781873	3610.249717	23.228608
106.975093	3617.552164	23.233626
106.529123	3630.294197	23.238643
106.949883	3617.995855	23.243661
106.657893	3609.847146	23.248679
106.771223	3621.146003	23.253696
106.901908	3644.102938	23.258714
106.986033	3640.967000	23.263731
107.697020	3649.478388	23.268749
107.431488	3646.051480	23.273767
107.705300	3633.785725	23.278784
108.024085	3637.578362	23.283802
107.605675	3642.367188	23.288819
108.066046	3645.165394	23.293837
108.347124	3665.906234	23.298855
108.384109	3653.982077	23.303872
108.519352	3670.991467	23.308890
108.653781	3669.460003	23.313907
108.799876	3663.967432	23.318925
108.650885	3664.959202	23.323943
108.691866	3660.216415	23.328960
108.753620	3659.562452	23.333978
108.674162	3650.403208	23.338995
109.256778	3656.162663	23.344013
108.790652	3654.465248	23.349031
109.017803	3657.405628	23.354048
108.628113	3664.762086	23.359066
108.791497	3678.522309	23.364083
108.977347	3680.729277	23.369101
109.006607	3688.164430	23.374119
109.147219	3695.445699	23.379136
109.400151	3707.325127	23.384154
109.463533	3718.875664	23.389171
109.580799	3718.471990	23.394189
109.738940	3736.670733	23.399207
110.264402	3720.271750	23.404224
110.205631	3727.929399	23.409242
110.368103	3730.796239	23.414259
110.660830	3731.021870	23.419277
110.778673	3729.426602	23.424295
110.885778	3716.192976	23.429312
111.067052	3744.951906	23.434330
111.242304	3756.843053	23.439347
111.618734	3751.287508	23.444365
111.672293	3757.788230	23.449383
111.683728	3744.230611	23.454400
111.356960	3745.068724	23.459418
111.532777	3744.142688	23.464435
111.412996	3749.351062	23.469453
111.503953	3749.901873	23.474471
112.009074	3736.742506	23.479488
111.632535	3750.954048	23.484506
111.855553	3763.829158	23.489523
112.081686	3769.753599	23.494541
111.941023	3783.638282	23.499559
112.141339	3782.590061	23.504576
112.577938	3786.980637	23.509594
112.717208	3814.001133	23.514611
112.693847	3808.512157	23.519629
112.845322	3815.605043	23.524647
113.107995	3801.889618	23.529664
113.170050	3805.883094	23.534682
112.872609	3810.443645	23.539699
112.960047	3809.786998	23.544717
112.860546	3826.209746	23.549735
113.367114	3820.592467	23.554752
113.578680	3826.901679	23.559770
113.673381	3849.848729	23.564787
113.961232	3843.595907	23.569805
114.021653	3851.661895	23.574823
114.259564	3845.645325	23.579840
114.306405	3843.348709	23.584858
113.979296	3847.087688	23.589875
114.734935	3856.246221	23.594893
114.496557	3872.419926	23.599911
114.687073	3878.570416	23.604928
114.771191	3869.869463	23.609946
115.001354	3879.421751	23.614963
115.186999	3881.789829	23.619981
114.863618	3874.136012	23.624999
115.144888	3886.629084	23.630016
115.378055	3899.286058	23.635034
115.305388	3908.857790	23.640051
115.841211	3906.449491	23.645069
115.823465	3910.473926	23.650087
115.768809	3903.599344	23.655104
115.896787	3912.648810	23.660122
116.122783	3930.749917	23.665139
116.411004	3935.903794	23.670157
116.549451	3932.281962	23.675175
116.442760	3933.440786	23.680192
116.619098	3933.487237	23.685210
116.239383	3936.547443	23.690227
116.797483	3928.938232	23.695245
116.618111	3927.788276	23.700263
116.711218	3938.320913	23.705280
117.114227	3942.112281	23.710298
117.025436	3960.483290	23.715315
117.525710	3963.304875	23.720333
117.411678	3962.668585	23.725351
117.493514	3955.832808	23.730368
117.484603	3960.344448	23.735386
117.362709	3963.804557	23.740403
118.082354	3977.765507	23.745421
117.959707	3983.802510	23.750439
118.043662	3993.212909	23.755456
118.332364	3986.160162	23.760474
118.174570	3997.127353	23.765491
118.390671	3994.820410	23.770509
118.493086	4017.725872	23.775527
118.506311	4017.882807	23.780544
119.080946	4016.011850	23.785562
118.800975	4019.282364	23.790579
119.250919	4012.728973	23.795597
119.290216	4019.153413	23.800615
119.265412	4018.720491	23.805632
119.319124	4023.398973	23.810650
119.521749	4035.132626	23.815667
119.670749	4030.515959	23.820685
119.721411	4035.669826	23.825703
119.711001	4030.490486	23.830720
120.221068	4042.089764	23.835738
120.087829	4049.819357	23.840755
120.630272	4061.965343	23.845773
120.905305	4065.104599	23.850791
121.150663	4058.185788	23.855808
120.956505	4051.841403	23.860826
120.957105	4060.441106	23.865843
121.235689	4044.965082	23.870861
121.195280	4048.399119	23.875879
121.385873	4054.922952	23.880896
121.376447	4045.064768	23.885914
121.158119	4048.866898	23.890931
121.216470	4045.719790	23.895949
121.338900	4052.017076	23.900967
121.048277	4066.478498	23.905984
121.613075	4069.636718	23.911002
121.686821	4083.193601	23.916019
122.129700	4094.214974	23.921037
122.126502	4110.484257	23.926055
122.193334	4118.728089	23.931072
122.488009	4115.236280	23.936090
122.384702	4123.064907	23.941107
122.318733	4127.905778	23.946125
122.779484	4132.423972	23.951143
122.546320	4140.999421	23.956160
123.289041	4125.772508	23.961178
123.026354	4148.297595	23.966195
123.133876	4157.250574	23.971213
123.432818	4164.840153	23.976231
123.254480	4164.345232	23.981248
123.965178	4150.912863	23.986266
123.820241	4170.620399	23.991283
124.042939	4179.540933	23.996301
124.071855	4183.833741	24.001319
124.387677	4189.773026	24.006336
124.491081	4181.042719	24.011354
124.583727	4183.510507	24.016371
124.521294	4184.428912	24.021389
124.414282	4182.239229	24.026407
124.387573	4183.573048	24.031424
124.838815	4197.244722	24.036442
124.784513	4209.766049	24.041459
124.875269	4209.674678	24.046477
125.137458	4219.685728	24.051495
125.046738	4219.444059	24.056512
125.342766	4221.087497	24.061530
125.024659	4240.818280	24.066547
125.136410	4246.395245	24.071565
125.656264	4255.311512	24.076583
125.423698	4262.975752	24.081600
126.092705	4258.659601	24.086618
125.927151	4273.717932	24.091635
126.305544	4276.562117	24.096653
126.644025	4294.108316	24.101671
126.677546	4295.890517	24.106688
126.957169	4287.464891	24.111706
127.123309	4294.367739	24.116723
127.227034	4283.559017	24.121741
127.137961	4280.980458	24.126759
126.675300	4293.095367	24.131776
127.412600	4303.175076	24.136794
127.487915	4310.213463	24.141811
127.655373	4314.800746	24.146829
127.790363	4317.227680	24.151847
127.654846	4316.438213	24.156864
127.909165	4327.056250	24.161882
128.261330	4348.274892	24.166899
128.108855	4334.104027	24.171917
128.423671	4333.922793	24.176935
128.126727	4343.749284	24.181952
128.692931	4343.697324	24.186970
128.848716	4363.739630	24.191987
128.947782	4364.139095	24.197005
129.120441	4359.572755	24.202023
129.168937	4364.025391	24.207040
129.366815	4358.569683	24.212058
129.391491	4384.598543	24.217075
129.420517	4387.291895	24.222093
129.636691	4386.970272	24.227111
129.917672	4393.241445	24.232128
129.921966	4384.283297	24.237146
129.652277	4411.980122	24.242163
129.835864	4412.229349	24.247181
130.078235	4418.469122	24.252199
130.158614	4434.583146	24.257216
130.188545	4441.008522	24.262234
130.386304	4440.678921	24.267251
130.497845	4454.074721	24.272269
130.925784	4468.469519	24.277287
130.908676	4477.904029	24.282304
131.027591	4476.140763	24.287322
131.016237	4491.531316	24.292339
131.481321	4502.757214	24.297357
131.485677	4491.314288	24.302375
131.570185	4501.810138	24.307392
132.025671	4515.461700	24.312410
132.187030	4526.744202	24.317427
132.304915	4526.862551	24.322445
132.734026	4524.017810	24.327463
132.589100	4526.792752	24.332480
132.818153	4519.882740	24.337498
132.946793	4525.875195	24.342515
132.972181	4523.714734	24.347533
132.999317	4517.468191	24.352551
133.132106	4528.181303	24.357568
133.406193	4535.337302	24.362586
133.504536	4543.056359	24.367603
133.505298	4550.773463	24.372621
133.685657	4548.104573	24.377639
133.515971	4547.722401	24.382656
133.649760	4543.363269	24.387674
133.728814	4559.095679	24.392691
134.191968	4573.895056	24.397709
133.991771	4573.168263	24.402727
133.882350	4575.416765	24.407744
134.276503	4572.751852	24.412762
134.059945	4588.680507	24.417779
134.528826	4601.184041	24.422797
135.212364	4603.297322	24.427815
134.846680	4603.696560	24.432832
135.152311	4621.916408	24.437850
135.107797	4641.774081	24.442867
135.381347	4632.522346	24.447885
135.594803	4625.804670	24.452903
135.404381	4639.452237	24.457920
135.897668	4651.508378	24.462938
136.084908	4647.827901	24.467955
136.201922	4655.649455	24.472973
136.357748	4652.515228	24.477991
136.105757	4653.383138	24.483008
136.396055	4672.668781	24.488026
137.080288	4680.918584	24.493043
137.053963	4685.495532	24.498061
137.224428	4679.800897	24.503079
136.911246	4690.600558	24.508096
136.957975	4678.594467	24.513114
137.151605	4694.262365	24.518131
137.367520	4704.874416	24.523149
137.504417	4705.381034	24.528167
137.451130	4718.432623	24.533184
138.303667	4723.370472	24.538202
137.971346	4742.909709	24.543219
137.985518	4737.966271	24.548237
138.138599	4741.863009	24.553255
137.941033	4751.656760	24.558272
138.427465	4764.222099	24.563290
138.460564	4757.078232	24.568307
138.773971	4773.894327	24.573325
138.898152	4786.970932	24.578343
139.176485	4796.640240	24.583360
139.142346	4800.775906	24.588378
139.506351	4796.595956	24.593395
139.306385	4812.895394	24.598413
139.705674	4820.330855	24.603431
139.535185	4829.928006	24.608448
139.778509	4835.064414	24.613466
140.151920	4845.344910	24.618483
140.053977	4851.250569	24.623501
140.505508	4850.992355	24.628519
140.619127	4858.220748	24.633536
140.907821	4863.522130	24.638554
141.032432	4870.844005	24.643571
141.362270	4871.705378	24.648589
141.583260	4868.416196	24.653607
141.758405	4869.832424	24.658624
141.553684	4858.719971	24.663642
141.980074	4863.542556	24.668659
141.708229	4865.927462	24.673677
141.810772	4856.125050	24.678695
142.025049	4855.990386	24.683712
142.186513	4873.989465	24.688730
142.342303	4884.794307	24.693747
141.988620	4886.126403	24.698765
142.411038	4883.411081	24.703783
142.186818	4889.399091	24.708800
142.518097	4909.613080	24.713818
142.644179	4920.770971	24.718835
142.510878	4922.984885	24.723853
142.972427	4937.224912	24.728871
142.891927	4948.439864	24.733888
143.208762	4949.230151	24.738906
143.522349	4957.493426	24.743923
143.684323	4974.882169	24.748941
144.170511	4976.517046	24.753959
144.074718	4976.131291	24.758976
144.025025	4978.152592	24.763994
144.093357	4975.685683	24.769011
144.342665	5004.304134	24.774029
144.687500	5004.462882	24.779047
144.777169	5002.046778	24.784064
144.822495	5007.482222	24.789082
144.926516	5013.786881	24.794099
144.902575	5026.554278	24.799117
145.142878	5035.162082	24.804135
145.749212	5039.473723	24.809152
145.748629	5053.535983	24.814170
146.004544	5056.198186	24.819187
146.150297	5068.976901	24.824205
146.362365	5062.786945	24.829223
146.309158	5059.921943	24.834240
146.424339	5060.005304	24.839258
146.421363	5069.400025	24.844275
146.435108	5071.962137	24.849293
146.734240	5079.328459	24.854311
146.657359	5073.573037	24.859328
147.072924	5089.553481	24.864346
147.365457	5102.293745	24.869363
147.402925	5104.321896	24.874381
147.306663	5109.428771	24.879399
147.807151	5117.807676	24.884416
147.638316	5129.990350	24.889434
148.016176	5123.030236	24.894451
147.807299	5140.054482	24.899469
148.437102	5143.754257	24.904487
148.364487	5153.386592	24.909504
148.287751	5165.435120	24.914522
148.588421	5163.935454	24.919539
148.360858	5174.658262	24.924557
148.909409	5178.966908	24.929575
148.710797	5200.056581	24.934592
149.162365	5214.770274	24.939610
149.459441	5218.240050	24.944627
149.023437	5229.271484	24.949645
149.599495	5229.710137	24.954663
149.848606	5245.241810	24.959680
149.836412	5253.608796	24.964698
150.071934	5257.668433	24.969715
150.089961	5279.424869	24.974733
150.550967	5280.643379	24.979751
150.750160	5281.048343	24.984768
150.711603	5290.917699	24.989786
151.040590	5298.999035	24.994803
150.925690	5306.660050	24.999821
151.341375	5314.021362	25.004839
151.226372	5309.715812	25.009856
151.381961	5325.783643	25.014874
152.002821	5328.857236	25.019891
152.110927	5339.507256	25.024909
152.399123	5338.254578	25.029927
152.687560	5337.116848	25.034944
152.321129	5332.527645	25.039962
152.760051	5320.000120	25.044979
152.736705	5347.018279	25.049997
152.998144	5355.522737	25.055015
152.933713	5371.096994	25.060032
152.638902	5360.876476	25.065050
153.161679	5357.520689	25.070067
153.121579	5378.500872	25.075085
153.340059	5388.608904	25.080103
153.615320	5407.118224	25.085120
153.449554	5406.826740	25.090138
153.962058	5404.046011	25.095155
154.077321	5426.185859	25.100173
153.799509	5430.402988	25.105191
154.259544	5420.825360	25.110208
154.527669	5444.088235	25.115226
154.825634	5448.139158	25.120243
154.567274	5452.073476	25.125261
154.753989	5446.030123	25.130279
155.113254	5469.182647	25.135296
155.293031	5476.364142	25.140314
155.705453	5468.586934	25.145331
155.472753	5476.231304	25.150349
155.756843	5495.725335	25.155367
156.046193	5498.317496	25.160384
156.110129	5499.007917	25.165402
156.475442	5504.228311	25.170419
156.470127	5514.775149	25.175437
156.729948	5519.198639	25.180455
156.806237	5519.359325	25.185472
156.456603	5521.368922	25.190490
157.067784	5529.565114	25.195507
157.008071	5545.166327	25.200525
157.113555	5544.321143	25.205543
157.362526	5560.242224	25.210560
157.469605	5562.244733	25.215578
157.798005	5567.886324	25.220595
158.095631	5571.502581	25.225613
158.123943	5595.065290	25.230631
158.469690	5598.193150	25.235648
158.533764	5607.131308	25.240666
158.641809	5600.492893	25.245683
158.874648	5616.773485	25.250701
158.954098	5631.127811	25.255719
159.158076	5621.905133	25.260736
158.937574	5630.043747	25.265754
159.164292	5642.359015	25.270771
159.727243	5663.187753	25.275789
159.530285	5665.641501	25.280807
159.863706	5671.817082	25.285824
160.215280	5690.688213	25.290842
160.148932	5683.480056	25.295859
160.415473	5697.193861	25.300877
160.832273	5689.502457	25.305895
160.794111	5710.255929	25.310912
160.815650	5718.557718	25.315930
161.014929	5719.011512	25.320947
161.435559	5720.673078	25.325965
161.786114	5721.631886	25.330983
162.131737	5734.212654	25.336000
162.452286	5739.001840	25.341018
162.242909	5738.252881	25.346035
162.269867	5746.481328	25.351053
162.522309	5739.447985	25.356071
162.617713	5731.867266	25.361088
162.684180	5739.733957	25.366106
162.725273	5731.011536	25.371123
162.644204	5729.357639	25.376141
163.136123	5747.280165	25.381159
163.523382	5756.760333	25.386176
163.317422	5770.453190	25.391194
163.421533	5762.761538	25.396211
163.548997	5762.278942	25.401229
163.712002	5779.889721	25.406247
163.995440	5793.534654	25.411264
163.666052	5798.184940	25.416282
163.917548	5783.177179	25.421299
164.111815	5801.757868	25.426317
164.323767	5818.750189	25.431335
164.664267	5818.840358	25.436352
164.483892	5839.230827	25.441370
164.957427	5847.528737	25.446387
164.949589	5855.994560	25.451405
164.943538	5872.281887	25.456423
165.312930	5879.009225	25.461440
165.220002	5887.184345	25.466458
165.508635	5899.821937	25.471475
166.007726	5911.358264	25.476493
165.439657	5924.612643	25.481511
166.109280	5932.208660	25.486528
166.114456	5948.235867	25.491546
166.377236	5960.803752	25.496563
166.961303	5969.617433	25.501581
167.056411	5972.218991	25.506599
167.305323	5974.692696	25.511616
167.488993	5987.799830	25.516634
167.803878	5987.787913	25.521651
168.081781	5995.630753	25.526669
168.137930	5994.409355	25.531687
168.170744	5994.882842	25.536704
168.308271	6011.382039	25.541722
168.406511	6014.823478	25.546739
168.472061	6014.192813	25.551757
168.891030	6014.252665	25.556775
169.077248	6042.166710	25.561792
168.861963	6054.026982	25.566810
168.949799	6053.610798	25.571827
169.126396	6054.624420	25.576845
169.473836	6069.740515	25.581863
169.686921	6067.955970	25.586880
169.850634	6083.867279	25.591898
170.389844	6103.233186	25.596915
170.688900	6099.932402	25.601933
170.463250	6112.178795	25.606951
170.672624	6099.109757	25.611968
170.769220	6124.505781	25.616986
170.906667	6128.048658	25.622003
171.273165	6136.468409	25.627021
171.392255	6135.920241	25.632039
171.701570	6148.345887	25.637056
171.761691	6172.216091	25.642074
171.833760	6165.220299	25.647091
172.027116	6161.904709	25.652109
171.635102	6178.943062	25.657127
172.429559	6186.001063	25.662144
172.209840	6195.638696	25.667162
172.292261	6201.515785	25.672180
172.570216	6208.653794	25.677197
172.680748	6219.637174	25.682215
173.189114	6236.456425	25.687232
172.994636	6244.382321	25.692250
172.948044	6250.784085	25.697268
173.794808	6269.532970	25.702285
173.589036	6273.350877	25.707303
174.215809	6287.055178	25.712320
174.291059	6295.980848	25.717338
174.282658	6309.446916	25.722356
174.935718	6307.096444	25.727373
174.855109	6305.532989	25.732391
175.043343	6305.197844	25.737408
175.001837	6322.877742	25.742426
175.320994	6327.422386	25.747444
175.542091	6331.377572	25.752461
175.534036	6334.429470	25.757479
175.884323	6326.905512	25.762496
175.741658	6338.641341	25.767514
176.090658	6357.156897	25.772532
176.281052	6354.030003	25.777549
176.319338	6363.763648	25.782567
176.836189	6368.223589	25.787584
176.736884	6388.284711	25.792602
176.993619	6377.811541	25.797620
177.426573	6382.877681	25.802637
177.301895	6410.114491	25.807655
177.622193	6403.204309	25.812672
177.793196	6401.859897	25.817690
178.181656	6405.744861	25.822708
178.299077	6404.540855	25.827725
178.090680	6423.496119	25.832743
178.460011	6426.691131	25.837760
178.362115	6431.854624	25.842778
178.603481	6447.541568	25.847796
178.895399	6458.428134	25.852813
179.162594	6459.711911	25.857831
179.593877	6462.053896	25.862848
179.756632	6479.111782	25.867866
179.830708	6493.969511	25.872884
180.120089	6492.908736	25.877901
180.181652	6493.540521	25.882919
180.318728	6489.679679	25.887936
180.546953	6501.192758	25.892954
180.415383	6528.976752	25.897972
181.094015	6515.198779	25.902989
180.788205	6532.414636	25.908007
181.012281	6536.494617	25.913024
181.463157	6553.190613	25.918042
180.968694	6563.489106	25.923060
181.332637	6573.261120	25.928077
181.495963	6590.894016	25.933095
181.374765	6599.134044	25.938112
181.807497	6617.955830	25.943130
181.986897	6630.219842	25.948148
182.307534	6638.603346	25.953165
182.531844	6649.191690	25.958183
182.416365	6662.485961	25.963200
183.148726	6676.119560	25.968218
183.172224	6685.606164	25.973236
183.397446	6695.613098	25.978253
183.847028	6712.524506	25.983271
183.895778	6709.119321	25.988288
184.137980	6734.721426	25.993306
183.947253	6738.380996	25.998324
184.393924	6732.424083	26.003341
184.382170	6737.729370	26.008359
184.511350	6757.803541	26.013376
185.057933	6757.138895	26.018394
184.583214	6778.668631	26.023412
185.480779	6787.066974	26.028429
185.357069	6784.110935	26.033447
185.925415	6804.242423	26.038464
186.005322	6809.949232	26.043482
186.270569	6816.913185	26.048500
186.433581	6818.756152	26.053517
186.339340	6826.032463	26.058535
186.607197	6838.615172	26.063552
186.924587	6848.742423	26.068570
186.889290	6848.875126	26.073588
187.224675	6848.968516	26.078605
187.304496	6859.273733	26.083623
187.610727	6863.655263	26.088640
187.701977	6867.812456	26.093658
187.261193	6870.779352	26.098676
187.891738	6886.186480	26.103693
187.936335	6895.935947	26.108711
188.042982	6912.024521	26.113728
188.488203	6922.001479	26.118746
188.117335	6928.321722	26.123764
188.386307	6942.092918	26.128781
188.364917	6969.815332	26.133799
188.952932	6982.498748	26.138816
189.135201	6985.322345	26.143834
189.255241	7020.846144	26.148852
189.842354	7020.700944	26.153869
189.996254	7036.833808	26.158887
190.211317	7049.483713	26.163904
190.661465	7047.536937	26.168922
190.519079	7073.670348	26.173940
191.450505	7073.891914	26.178957
191.400489	7089.782905	26.183975
191.766922	7088.638446	26.188992
191.802095	7085.544197	26.194010
191.676222	7093.837241	26.199028
192.005233	7109.185808	26.204045
192.242489	7110.710112	26.209063
192.091407	7115.554959	26.214080
192.557820	7120.084118	26.219098
192.622684	7139.654280	26.224116
192.626871	7140.909190	26.229133
192.888641	7153.157607	26.234151
193.193478	7169.239624	26.239168
193.676737	7164.205168	26.244186
193.471420	7181.976156	26.249204
193.439536	7190.338759	26.254221
193.620161	7201.404950	26.259239
193.919173	7221.368097	26.264256
194.053755	7223.537980	26.269274
194.152146	7249.589283	26.274292
194.644546	7250.813789	26.279309
194.804840	7274.178339	26.284327
194.966981	7292.191087	26.289344
195.627771	7290.058964	26.294362
195.374938	7305.148800	26.299380
195.485174	7320.753555	26.304397
195.903763	7331.704823	26.309415
196.310079	7338.594453	26.314432
196.593191	7343.725884	26.319450
196.320203	7348.346799	26.324468
196.391930	7350.181310	26.329485
196.746963	7368.400093	26.334503
197.056749	7370.132967	26.339520
197.198843	7385.496205	26.344538
197.082337	7399.374151	26.349556
197.753128	7414.651466	26.354573
197.963161	7422.492074	26.359591
198.110295	7432.294212	26.364608
198.442842	7432.414072	26.369626
198.438476	7440.086171	26.374644
198.854805	7456.706133	26.379661
198.789246	7457.372392	26.384679
199.131145	7481.778445	26.389696
199.473563	7478.113377	26.394714
199.773070	7498.780203	26.399732
199.784785	7492.937552	26.404749
200.026997	7502.605839	26.409767
199.923615	7522.603686	26.414784
200.487527	7514.109600	26.419802
200.266674	7522.059400	26.424820
200.631076	7531.362465	26.429837
200.536736	7547.871715	26.434855
200.276723	7555.321527	26.439872
200.991707	7566.364887	26.444890
200.779949	7578.564418	26.449908
201.269584	7598.048281	26.454925
201.500197	7623.060598	26.459943
201.468578	7630.061453	26.464960
201.994296	7636.045282	26.469978
202.113020	7655.071524	26.474996
202.401011	7665.270332	26.480013
202.910020	7677.268694	26.485031
202.737713	7697.981591	26.490048
203.043922	7702.119959	26.495066
203.797531	7712.101503	26.500084
203.985300	7718.743905	26.505101
204.055659	7735.580551	26.510119
204.141124	7737.348241	26.515136
204.787592	7729.843912	26.520154
204.303148	7740.176159	26.525172
204.752346	7755.683477	26.530189
204.635792	7759.894211	26.535207
205.105844	7782.898659	26.540224
205.252101	7790.050522	26.545242
205.447621	7804.738130	26.550260
205.548579	7813.029442	26.555277
205.670174	7818.935305	26.560295
205.666570	7841.091115	26.565312
206.214778	7839.506116	26.570330
206.342051	7858.349224	26.575348
206.227343	7876.833831	26.580365
206.644795	7891.942440	26.585383
206.973715	7914.338696	26.590400
207.117693	7912.659916	26.595418
207.447239	7936.181743	26.600436
207.711042	7949.057461	26.605453
207.899507	7962.310374	26.610471
207.865879	7973.310956	26.615488
208.425917	7979.024561	26.620506
208.680423	7996.573816	26.625524
208.656567	7995.480518	26.630541
208.918641	8007.946955	26.635559
209.215348	8036.552011	26.640576
209.781586	8035.112889	26.645594
209.726983	8045.820810	26.650612
209.973144	8055.272156	26.655629
210.205476	8065.733295	26.660647
210.251505	8068.057381	26.665664
210.306894	8087.794122	26.670682
210.478088	8093.392541	26.675700
210.937480	8108.001298	26.680717
210.932856	8125.798402	26.685735
211.312537	8136.080799	26.690752
211.557369	8145.955428	26.695770
211.865703	8150.729258	26.700788
211.989988	8163.417135	26.705805
212.219268	8176.111272	26.710823
212.496372	8179.057237	26.715840
212.596824	8185.091196	26.720858
212.675536	8209.066147	26.725876
212.932881	8218.653591	26.730893
213.393851	8225.296667	26.735911
213.438933	8249.323721	26.740928
213.879460	8243.859602	26.745946
213.963737	8251.741920	26.750964
214.356190	8272.524340	26.755981
214.638937	8267.086333	26.760999
214.751811	8278.236961	26.766016
214.876403	8265.729236	26.771034
214.717622	8273.430450	26.776052
215.305912	8285.042763	26.781069
215.601281	8288.407162	26.786087
215.657186	8291.248762	26.791104
215.906909	8304.892777	26.796122
216.068157	8311.207394	26.801140
216.247675	8312.819361	26.806157
216.494918	8317.934203	26.811175
216.403795	8335.781309	26.816192
217.015424	8352.413203	26.821210
216.607182	8349.040785	26.826228
216.962459	8384.032406	26.831245
217.241445	8387.011183	26.836263
217.323605	8408.477702	26.841280
217.333384	8421.528195	26.846298
217.740955	8434.894900	26.851316
217.659342	8457.640318	26.856333
218.311296	8467.755756	26.861351
218.401449	8499.453068	26.866368
219.116232	8507.569077	26.871386
219.166124	8511.226240	26.876404
219.124385	8529.087442	26.881421
219.440581	8532.502012	26.886439
219.737432	8561.398665	26.891456
220.186854	8570.568528	26.896474
220.437089	8583.925956	26.901492
220.605404	8590.710588	26.906509
220.830874	8596.909916	26.911527
220.875774	8619.778778	26.916544
221.124002	8629.156863	26.921562
221.323729	8637.978952	26.926580
221.801164	8652.584435	26.931597
222.186757	8647.086737	26.936615
222.444236	8672.292403	26.941632
222.534985	8678.035899	26.946650
222.870921	8678.043353	26.951668
222.723376	8694.561018	26.956685
223.367360	8709.601394	26.961703
223.494058	8719.603859	26.966720
223.655769	8717.729061	26.971738
223.492249	8732.917317	26.976756
223.324319	8755.906684	26.981773
223.947756	8771.920249	26.986791
224.008726	8785.762926	26.991808
224.096634	8792.143443	26.996826
224.631857	8811.122595	27.001844
224.605778	8835.416756	27.006861
225.153849	8843.549508	27.011879
225.296625	8860.313118	27.016896
225.560164	8868.844328	27.021914
225.800439	8886.613553	27.026932
225.948488	8907.196992	27.031949
226.345317	8902.403184	27.036967
226.487037	8934.012467	27.041984
226.792906	8929.796961	27.047002
227.117208	8954.625699	27.052020
227.179103	8962.760220	27.057037
227.668797	8976.530514	27.062055
227.585811	9008.690767	27.067072
227.792251	9002.087431	27.072090
228.460445	9017.978821	27.077108
228.555609	9039.220306	27.082125
229.019070	9032.581500	27.087143
228.953487	9058.161877	27.092160
229.347252	9066.479419	27.097178
229.801421	9067.060494	27.102196
229.513047	9075.440546	27.107213
230.021159	9070.413993	27.112231
229.744631	9093.560469	27.117248
229.758791	9099.335703	27.122266
230.315073	9118.353487	27.127284
230.155714	9127.707956	27.132301
230.592500	9144.895070	27.137319
230.776990	9162.296491	27.142336
231.217754	9171.224712	27.147354
231.287093	9184.840257	27.152372
231.752395	9195.690547	27.157389
232.039324	9211.568831	27.162407
232.345304	9225.073548	27.167424
232.442995	9233.395286	27.172442
232.617115	9245.607831	27.177460
233.059558	9256.308329	27.182477
233.264833	9262.489990	27.187495
233.380936	9281.376014	27.192512
233.447947	9288.306121	27.197530
233.727175	9301.653836	27.202548
233.881234	9315.695838	27.207565
234.141318	9323.419596	27.212583
234.530436	9346.297111	27.217600
234.781468	9363.747607	27.222618
234.783414	9369.677003	27.227636
234.936396	9391.258372	27.232653
235.382831	9401.824384	27.237671
235.567848	9428.811034	27.242688
235.734364	9436.748860	27.247706
236.174669	9447.190657	27.252724
236.389007	9473.959826	27.257741
236.671854	9488.695187	27.262759
237.042648	9503.438061	27.267776
237.424306	9516.243540	27.272794
237.778386	9525.191824	27.277812
237.685360	9531.224447	27.282829
238.122532	9546.900151	27.287847
238.079810	9557.148616	27.292864
238.382031	9576.207428	27.297882
238.803752	9589.282850	27.302900
238.582815	9595.050700	27.307917
238.741326	9611.610815	27.312935
238.874827	9635.423633	27.317952
239.062230	9647.151363	27.322970
239.749026	9671.954293	27.327988
239.621973	9686.288949	27.333005
240.181321	9707.415875	27.338023
240.350367	9719.030102	27.343040
240.713882	9740.346263	27.348058
241.339162	9745.209911	27.353076
241.479114	9757.337905	27.358093
242.191422	9770.633225	27.363111
242.300345	9764.659423	27.368128
242.263601	9765.688912	27.373146
242.731287	9780.157601	27.378164
242.715860	9799.162908	27.383181
242.864834	9795.706601	27.388199
243.640174	9809.268040	27.393216
243.399789	9822.946427	27.398234
243.730526	9827.224674	27.403252
243.913579	9839.804887	27.408269
244.331119	9855.726002	27.413287
244.363461	9854.862768	27.418304
244.517568	9873.476129	27.423322
245.033578	9880.172239	27.428340
244.989875	9890.468348	27.433357
244.928946	9896.382349	27.438375
245.305210	9908.769918	27.443392
245.520005	9918.906657	27.448410
245.745858	9925.854863	27.453428
245.822597	9942.951177	27.458445
245.638917	9961.840358	27.463463
246.122970	9978.179156	27.468480
246.176113	10005.969333	27.473498
246.665253	10012.208285	27.478516
246.338417	10049.135534	27.483533
246.599165	10060.511086	27.488551
246.842435	10086.239714	27.493568
246.957769	10112.371655	27.498586
247.565955	10134.872903	27.503604
247.655162	10173.619979	27.508621
248.241068	10188.546103	27.513639
248.601336	10218.638257	27.518656
248.815402	10247.762003	27.523674
249.305389	10259.113930	27.528692
249.347241	10273.848151	27.533709
249.606741	10290.794830	27.538727
250.588038	10295.122289	27.543744
250.413703	10320.435903	27.548762
250.808070	10333.984435	27.553780
250.943634	10341.281809	27.558797
251.549166	10361.282440	27.563815
251.848306	10363.022929	27.568832
252.005188	10382.232023	27.573850
252.643385	10387.222150	27.578868
252.480702	10391.366362	27.583885
252.631863	10414.456539	27.588903
252.880729	10414.643073	27.593920
253.106114	10451.683090	27.598938
253.535675	10452.937962	27.603956
253.489032	10468.803381	27.608973
253.630531	10487.382510	27.613991
253.867132	10494.821585	27.619008
253.667563	10517.022981	27.624026
254.451040	10538.604728	27.629044
254.491734	10553.820770	27.634061
254.804918	10579.778905	27.639079
255.304456	10589.615245	27.644096
255.422920	10612.451129	27.649114
256.184556	10631.704587	27.654132
255.886460	10651.555781	27.659149
256.333907	10658.441623	27.664167
256.801939	10682.343214	27.669184
256.636425	10701.145163	27.674202
257.277636	10712.289596	27.679220
257.523402	10724.686006	27.684237
257.448244	10749.916120	27.689255
258.021667	10755.717547	27.694272
258.133792	10772.839610	27.699290
258.577123	10778.309621	27.704308
259.006183	10799.178288	27.709325
259.010217	10814.235194	27.714343
259.448667	10828.860939	27.719360
259.368540	10841.188479	27.724378
259.852330	10849.048485	27.729396
260.016130	10877.422193	27.734413
260.196804	10879.908758	27.739431
260.558981	10896.776837	27.744448
260.647218	10918.809812	27.749466
261.194302	10935.644171	27.754484
261.280971	10951.116124	27.759501
261.405553	10968.521538	27.764519
261.669550	10978.364018	27.769536
261.964886	11004.889904	27.774554
262.319145	11013.329242	27.779572
262.608970	11019.793824	27.784589
262.810296	11045.265414	27.789607
263.212442	11043.722425	27.794624
262.963363	11064.626481	27.799642
263.492925	11074.021670	27.804660
263.929818	11102.356870	27.809677
264.050118	11109.015003	27.814695
264.783071	11116.080689	27.819712
264.579048	11130.806758	27.824730
264.776034	11137.477421	27.829748
265.382831	11160.909239	27.834765
265.407613	11164.642860	27.839783
266.005755	11182.515324	27.844800
265.697683	11199.576609	27.849818
266.169157	11220.060620	27.854836
266.714089	11228.531539	27.859853
266.824261	11252.453820	27.864871
266.905929	11261.619139	27.869888
266.971937	11279.029857	27.874906
267.369650	11286.932691	27.879924
267.538979	11311.888421	27.884941
267.703737	11337.546162	27.889959
268.390968	11347.189595	27.894976
268.278489	11375.966036	27.899994
268.486266	11388.002089	27.905012
268.602499	11405.615783	27.910029
269.012650	11438.097130	27.915047
269.363337	11455.164668	27.920064
269.747234	11479.220036	27.925082
270.202911	11488.857762	27.930100
270.743876	11508.468685	27.935117
270.638198	11536.196388	27.940135
271.241727	11537.795227	27.945152
271.581525	11561.311219	27.950170
271.887660	11572.781179	27.955188
272.208471	11581.489510	27.960205
272.153196	11602.445694	27.965223
272.639122	11606.010110	27.970240
272.908944	11626.370439	27.975258
272.828432	11640.868519	27.980276
273.302955	11668.416889	27.985293
273.691719	11685.750981	27.990311
274.271444	11697.733575	27.995328
274.289685	11713.932997	28.000346
274.341688	11730.859596	28.005364
274.638265	11738.620237	28.010381
275.170827	11773.220362	28.015399
275.475423	11781.124671	28.020416
275.790863	11797.982520	28.025434
276.011773	11804.342216	28.030452
276.442729	11821.771897	28.035469
276.671470	11837.339365	28.040487
277.217257	11832.116637	28.045504
277.390172	11837.768872	28.050522
277.798895	11863.029352	28.055540
277.445859	11861.505716	28.060557
277.772978	11889.567366	28.065575
278.052515	11890.909437	28.070592
277.899826	11917.227335	28.075610
278.299204	11934.939710	28.080628
278.565595	11952.849035	28.085645
278.830401	11976.195249	28.090663
279.002560	11994.169068	28.095680
278.830027	12025.490535	28.100698
279.281767	12046.878663	28.105716
280.063841	12071.571824	28.110733
280.128237	12095.744030	28.115751
280.348119	12118.997032	28.120768
280.940369	12131.991143	28.125786
281.055740	12149.968232	28.130804
281.634623	12161.510075	28.135821
281.640601	12183.043083	28.140839
281.839963	12194.126166	28.145856
282.525796	12213.641476	28.150874
282.414146	12235.881097	28.155892
283.137338	12243.015087	28.160909
283.199736	12263.672144	28.165927
283.413180	12271.621723	28.170944
283.814673	12294.610111	28.175962
283.994660	12299.295335	28.180980
284.361707	12315.410830	28.185997
284.593506	12336.260558	28.191015
284.415973	12357.269470	28.196032
285.177272	12381.709678	28.201050
285.332206	12390.831991	28.206068
285.722977	12422.729147	28.211085
285.931174	12425.862232	28.216103
286.020355	12453.833446	28.221120
286.520105	12473.710807	28.226138
286.092269	12483.002128	28.231156
287.060699	12512.744169	28.236173
287.210233	12536.277313	28.241191
287.320208	12549.345288	28.246208
287.876558	12579.896329	28.251226
288.161293	12606.116144	28.256244
288.523080	12615.049905	28.261261
288.620287	12637.567529	28.266279
288.969239	12670.898276	28.271296
289.515795	12689.635085	28.276314
289.546268	12711.252988	28.281332
289.860910	12728.403478	28.286349
290.256989	12752.595824	28.291367
290.577469	12761.063733	28.296384
291.115727	12795.893605	28.301402
291.050765	12802.624075	28.306420
291.822231	12821.924229	28.311437
291.915726	12845.120395	28.316455
292.525939	12867.841811	28.321472
292.802056	12878.715667	28.326490
293.104548	12893.211350	28.331508
293.536415	12899.430971	28.336525
293.322413	12919.327742	28.341543
293.973397	12930.891295	28.346560
294.311809	12948.120031	28.351578
294.308954	12972.342493	28.356596
294.482980	12974.103983	28.361613
294.962614	13008.854187	28.366631
295.302190	13014.424088	28.371648
295.150424	13027.189068	28.376666
295.501037	13057.387384	28.381684
296.145377	13063.863447	28.386701
295.989431	13094.295395	28.391719
296.386099	13118.417271	28.396736
296.846568	13137.830742	28.401754
297.249475	13165.752825	28.406772
297.606453	13174.818495	28.411789
297.647042	13205.539611	28.416807
297.831480	13211.965784	28.421824
298.339109	13241.194458	28.426842
298.410520	13268.642069	28.431860
298.806554	13287.825264	28.436877
299.247368	13302.705012	28.441895
299.795580	13322.498170	28.446912
300.180448	13343.598069	28.451930
300.547260	13357.092239	28.456948
300.750757	13356.358874	28.461965
300.808036	13364.826538	28.466983
301.202251	13386.456045	28.472000
301.284360	13398.175561	28.477018
301.473306	13417.415251	28.482036
301.877690	13427.311631	28.487053
301.879620	13448.914748	28.492071
302.333261	13462.572718	28.497088
302.718514	13485.333812	28.502106
302.854962	13514.666968	28.507124
303.403377	13526.668713	28.512141
303.230649	13556.494395	28.517159
303.522042	13574.106660	28.522176
303.843294	13591.022144	28.527194
304.176023	13622.322928	28.532212
304.277758	13652.524143	28.537229
304.522287	13674.568079	28.542247
304.668524	13698.651891	28.547264
305.376432	13732.604648	28.552282
305.613642	13758.714408	28.557300
306.261445	13785.230623	28.562317
306.199946	13808.899822	28.567335
306.799656	13835.003285	28.572352
307.215398	13859.482431	28.577370
307.391253	13883.400860	28.582388
307.947467	13895.902758	28.587405
308.162269	13921.802150	28.592423
308.294924	13948.269939	28.597440
308.984994	13959.298217	28.602458
309.278637	13991.400491	28.607476
309.719311	13999.669486	28.612493
310.131374	14033.247888	28.617511
310.176347	14039.450037	28.622528
310.748808	14054.013964	28.627546
311.261306	14088.541961	28.632564
311.631406	14087.831421	28.637581
311.574534	14107.999920	28.642599
311.995129	14123.230493	28.647616
312.420836	14140.455497	28.652634
312.802879	14159.654643	28.657652
312.989348	14174.206919	28.662669
313.161238	14204.941275	28.667687
313.115080	14222.287023	28.672704
313.545995	14229.870595	28.677722
313.937174	14260.617614	28.682740
314.037247	14276.744571	28.687757
314.589915	14298.164661	28.692775
314.704128	14328.153865	28.697792
315.180494	14342.083046	28.702810
315.311708	14373.776389	28.707828
315.681086	14395.411344	28.712845
315.865086	14413.070659	28.717863
316.379955	14436.207216	28.722880
316.541044	14451.856153	28.727898
316.843250	14480.106062	28.732916
317.195653	14506.867778	28.737933
317.492778	14524.615661	28.742951
317.744227	14553.290181	28.747968
318.012400	14577.542656	28.752986
318.629601	14614.097030	28.758004
318.791905	14624.396707	28.763021
319.216207	14661.662409	28.768039
319.441756	14679.605133	28.773056
320.250947	14691.930228	28.778074
320.290371	14717.721211	28.783092
320.791678	14744.343614	28.788109
320.994689	14766.739481	28.793127
321.033908	14784.219844	28.798144
321.406749	14804.459919	28.803162
322.031415	14824.292681	28.808180
321.916617	14845.360595	28.813197
322.501016	14856.588227	28.818215
322.420706	14878.892446	28.823232
322.974053	14902.362157	28.828250
323.159063	14928.085241	28.833268
323.573586	14942.660344	28.838285
324.072932	14965.563802	28.843303
324.058419	14993.720439	28.848320
324.726743	15001.871882	28.853338
324.669859	15036.103667	28.858356
325.072560	15059.016948	28.863373
325.266623	15082.524319	28.868391
325.400040	15107.381473	28.873408
326.177174	15130.477177	28.878426
326.642005	15152.833388	28.883444
326.563607	15183.733941	28.888461
327.228813	15203.650293	28.893479
327.383281	15229.829681	28.898496
327.837039	15259.386109	28.903514
328.015818	15290.408213	28.908532
328.381777	15304.172080	28.913549
328.574460	15331.692911	28.918567
328.946616	15350.921886	28.923584
329.272012	15384.471691	28.928602
329.658817	15423.822703	28.933620
329.806406	15438.551185	28.938637
330.267737	15469.419680	28.943655
330.722994	15505.660818	28.948672
331.220596	15512.715391	28.953690
331.190547	15549.880204	28.958708
331.730069	15570.391531	28.963725
332.360368	15598.677324	28.968743
332.406840	15629.447711	28.973760
333.178853	15640.871800	28.978778
333.584294	15662.221897	28.983796
334.107564	15692.677057	28.988813
334.019417	15700.818508	28.993831
334.402288	15726.506939	28.998848
334.969464	15744.575543	29.003866
334.911242	15770.612884	29.008884
335.469154	15782.920502	29.013901
335.734563	15812.844830	29.018919
335.798661	15831.761254	29.023936
336.570181	15853.377280	29.028954
336.463373	15880.688526	29.033972
337.015740	15906.675457	29.038989
336.943703	15928.253094	29.044007
337.406172	15957.429468	29.049024
337.881740	15980.971915	29.054042
337.919563	16021.655697	29.059060
338.372505	16040.039863	29.064077
338.900795	16063.392436	29.069095
339.167923	16098.066152	29.074112
339.647110	16113.419705	29.079130
339.963652	16144.450562	29.084148
340.614424	16164.123002	29.089165
340.785432	16192.730153	29.094183
341.088261	16209.886249	29.099200
341.790998	16234.991338	29.104218
342.069974	16258.429588	29.109236
342.390773	16273.595138	29.114253
343.024902	16291.829802	29.119271
342.837182	16309.981417	29.124288
343.127897	16323.460682	29.129306
343.729520	16357.415978	29.134324
343.513637	16373.680826	29.139341
344.450460	16393.703410	29.144359
344.646508	16421.745666	29.149376
345.011496	16436.880409	29.154394
345.436893	16445.446358	29.159412
345.563201	16465.771843	29.164429
345.828271	16476.113993	29.169447
346.037307	16507.477002	29.174464
346.394050	16533.191506	29.179482
346.454511	16548.523347	29.184500
346.628877	16580.675639	29.189517
347.274326	16597.914142	29.194535
347.485062	16632.294091	29.199552
347.738346	16653.792031	29.204570
348.170757	16695.818200	29.209588
348.259285	16720.049971	29.214605
348.741650	16746.119168	29.219623
349.043916	16779.324127	29.224640
349.546070	16812.146130	29.229658
349.676901	16837.602156	29.234676
350.278734	16876.066687	29.239693
350.748251	16900.213594	29.244711
350.991666	16937.470246	29.249728
351.209503	16966.050490	29.254746
351.628382	16999.050583	29.259764
352.137114	17023.834314	29.264781
352.351346	17060.115606	29.269799
352.393650	17092.899206	29.274816
353.175789	17121.066325	29.279834
353.765601	17144.547386	29.284852
353.830194	17178.377298	29.289869
354.357306	17193.690824	29.294887
354.818999	17227.472450	29.299904
355.257350	17247.435133	29.304922
355.790894	17283.832731	29.309940
355.976712	17309.510524	29.314957
356.234697	17325.822401	29.319975
356.733610	17359.757348	29.324992
357.407921	17380.921720	29.330010
357.567043	17403.289021	29.335028
357.720013	17434.819123	29.340045
358.416361	17457.256790	29.345063
358.511093	17480.402537	29.350080
359.137103	17506.085019	29.355098
359.523189	17534.022038	29.360116
359.745209	17553.407690	29.365133
360.200176	17581.434276	29.370151
360.289395	17597.282527	29.375168
360.673850	17633.763895	29.380186
361.125429	17649.678331	29.385204
361.102158	17678.009654	29.390221
361.627375	17698.147668	29.395239
361.999557	17731.826909	29.400256
362.533036	17768.039567	29.405274
362.421284	17788.127054	29.410292
363.018652	17817.620153	29.415309
363.423701	17844.310785	29.420327
363.578206	17881.989404	29.425344
363.732334	17916.565820	29.430362
364.285373	17953.336841	29.435380
364.527563	17981.303158	29.440397
364.824767	18010.885691	29.445415
365.381381	18046.559148	29.450432
365.986601	18071.837657	29.455450
366.370847	18100.991348	29.460468
366.403374	18132.785474	29.465485
367.088478	18164.490569	29.470503
367.477222	18189.548130	29.475520
367.951692	18218.884147	29.480538
368.605525	18242.397155	29.485556
368.741577	18260.606082	29.490573
369.128927	18286.025021	29.495591
369.007974	18299.602406	29.500608
369.221147	18326.823723	29.505626
369.787468	18349.569456	29.510644
369.817754	18394.343270	29.515661
370.373489	18422.111823	29.520679
370.761970	18451.732054	29.525696
371.118885	18484.139997	29.530714
371.741791	18516.836611	29.535732
371.758856	18545.066567	29.540749
372.668077	18577.131047	29.545767
372.760006	18603.579923	29.550784
372.986035	18636.087071	29.555802
373.455060	18664.914000	29.560820
373.656939	18699.353288	29.565837
374.108536	18723.761203	29.570855
374.755748	18762.774359	29.575872
375.369869	18796.824018	29.580890
375.724297	18819.758382	29.585908
375.721430	18852.633320	29.590925
376.215971	18869.806157	29.595943
376.629013	18913.029808	29.600960
376.671423	18939.438540	29.605978
377.336585	18966.124179	29.610996
377.280558	18997.605119	29.616013
377.763679	19038.476394	29.621031
378.252488	19077.442407	29.626048
378.645984	19113.231853	29.631066
379.498885	19136.126717	29.636084
379.851956	19178.542769	29.641101
380.075554	19202.929213	29.646119
380.473139	19241.794045	29.651136
381.047202	19260.697757	29.656154
381.434994	19290.284907	29.661172
381.844773	19322.340468	29.666189
382.309641	19349.518640	29.671207
382.825685	19381.104262	29.676224
383.092957	19403.377518	29.681242
383.369180	19415.764425	29.686260
383.758979	19451.903623	29.691277
384.045109	19485.862353	29.696295
384.588740	19517.828344	29.701312
384.718988	19537.185772	29.706330
385.263388	19573.421039	29.711348
385.247795	19604.973677	29.716365
385.797696	19634.313887	29.721383
385.989501	19675.736279	29.726400
386.494273	19710.042381	29.731418
387.207279	19739.857129	29.736436
387.515620	19773.237317	29.741453
387.907911	19802.422602	29.746471
388.208970	19831.023936	29.751488
388.185760	19865.971120	29.756506
388.996974	19882.936508	29.761524
389.312053	19921.608464	29.766541
389.810843	19955.250739	29.771559
390.018477	19984.198881	29.776576
390.347253	20023.046958	29.781594
391.153396	20045.796304	29.786612
391.772812	20074.154596	29.791629
391.994144	20107.751655	29.796647
392.095633	20134.751599	29.801664
392.616478	20177.002092	29.806682
392.903974	20187.189910	29.811700
393.354246	20230.782878	29.816717
393.882181	20257.665143	29.821735
393.933429	20274.844998	29.826752
394.221486	20315.177782	29.831770
394.846131	20331.958508	29.836788
394.701450	20370.437985	29.841805
395.287686	20402.124278	29.846823
395.858260	20435.180165	29.851840
395.755086	20474.349882	29.856858
396.511784	20502.246295	29.861876
396.512537	20541.941333	29.866893
397.093707	20572.048988	29.871911
397.698802	20597.380220	29.876928
397.867392	20643.168271	29.881946
398.962314	20672.697587	29.886964
399.170659	20712.888427	29.891981
399.486291	20744.364732	29.896999
399.849176	20766.869933	29.902016
400.003339	20813.912709	29.907034
400.626593	20839.864085	29.912052
400.754857	20874.070905	29.917069
401.233472	20906.863866	29.922087
401.419847	20944.883080	29.927104
401.994331	20995.691287	29.932122
402.688385	21028.447254	29.937140
402.639017	21067.560564	29.942157
403.376767	21104.725765	29.947175
404.067405	21127.809460	29.952192
404.080695	21167.041920	29.957210
404.913756	21193.522002	29.962228
405.045934	21228.993410	29.967245
405.630523	21253.329391	29.972263
406.052400	21285.683118	29.977280
406.420462	21327.365786	29.982298
407.039236	21352.793648	29.987316
407.277986	21396.779403	29.992333
407.660707	21422.166024	29.997351
408.192578	21461.529353	30.002368
408.405241	21493.121854	30.007386
408.948346	21524.413755	30.012404
409.267450	21554.494009	30.017421
409.743896	21599.719687	30.022439
410.180396	21626.868398	30.027456
410.132570	21670.036657	30.032474
410.803986	21707.589432	30.037492
411.273135	21742.629304	30.042509
411.425937	21779.293633	30.047527
412.244928	21800.628881	30.052544
412.346927	21840.138343	30.057562
412.779733	21875.611809	30.062580
413.637166	21920.832056	30.067597
413.546889	21959.938430	30.072615
414.592109	21985.052269	30.077632
414.625851	22030.686643	30.082650
414.949152	22046.437283	30.087668
415.473773	22087.876742	30.092685
415.778360	22122.238234	30.097703
416.367633	22160.305451	30.102720
416.768130	22194.102492	30.107738
417.648942	22232.690847	30.112756
417.606134	22261.864098	30.117773
417.890168	22298.774312	30.122791
418.637100	22329.004314	30.127808
418.876903	22355.445646	30.132826
419.202537	22396.114616	30.137844
419.782654	22436.251176	30.142861
420.124429	22471.319944	30.147879
420.896236	22496.629594	30.152896
420.824319	22539.868701	30.157914
421.213722	22563.330620	30.162932
421.584805	22590.105379	30.167949
422.056260	22634.483154	30.172967
422.385035	22659.218287	30.177984
422.934704	22701.568091	30.183002
423.372473	22723.655103	30.188020
423.803693	22762.536677	30.193037
424.062536	22799.127316	30.198055
424.212249	22827.071266	30.203072
424.838590	22867.820901	30.208090
425.155219	22906.974067	30.213108
425.768729	22943.682930	30.218125
425.881215	22982.018545	30.223143
426.335805	23008.029552	30.228160
426.829263	23060.473661	30.233178
427.397494	23092.300440	30.238196
427.893944	23143.730375	30.243213
428.319121	23176.448273	30.248231
429.085374	23204.322345	30.253248
429.550600	23254.177737	30.258266
429.793785	23284.787692	30.263284
430.163341	23305.439156	30.268301
430.566679	23352.081892	30.273319
430.855292	23387.684880	30.278336
431.192636	23423.751374	30.283354
431.714677	23472.218203	30.288372
431.968662	23508.041633	30.293389
432.387881	23541.335217	30.298407
433.135819	23585.642909	30.303424
433.378474	23636.080292	30.308442
434.277700	23672.314517	30.313460
434.615208	23692.325211	30.318477
435.117927	23735.730868	30.323495
435.644932	23777.016357	30.328512
435.841478	23818.545869	30.333530
436.411526	23838.081436	30.338548
436.510949	23883.758788	30.343565
436.763039	23932.372525	30.348583
437.670972	23963.272655	30.353600
437.848576	24004.266432	30.358618
438.433202	24051.737369	30.363636
439.042957	24081.911193	30.368653
439.317387	24123.687180	30.373671
439.969124	24158.966749	30.378688
440.003574	24198.429780	30.383706
440.537129	24244.676505	30.388724
441.172771	24279.902216	30.393741
441.321302	24323.087277	30.398759
441.739761	24358.847423	30.403776
442.327261	24414.131340	30.408794
442.589931	24451.683706	30.413812
443.597008	24498.123997	30.418829
443.867387	24537.261747	30.423847
444.237299	24579.634926	30.428864
444.694675	24612.531605	30.433882
445.062557	24644.720882	30.438900
445.922142	24674.002814	30.443917
446.026561	24714.679226	30.448935
446.972586	24742.275318	30.453952
447.241062	24780.470873	30.458970
447.826897	24817.055877	30.463988
448.021995	24848.819944	30.469005
447.981569	24893.072249	30.474023
448.617395	24931.740390	30.479040
449.100092	24970.875534	30.484058
449.366598	25018.133698	30.489076
449.957650	25051.460137	30.494093
450.347660	25103.514443	30.499111
450.970351	25140.844723	30.504128
451.414436	25173.933928	30.509146
451.653681	25208.649943	30.514164
452.280526	25245.926143	30.519181
452.566980	25270.320374	30.524199
452.940946	25303.547600	30.529216
453.330217	25347.783585	30.534234
453.658407	25387.888348	30.539252
454.265430	25421.490431	30.544269
454.345483	25474.325773	30.549287
455.095967	25512.058374	30.554304
455.403134	25559.730807	30.559322
455.674638	25599.593107	30.564340
456.558874	25635.878137	30.569357
456.737906	25685.770622	30.574375
457.369483	25738.439800	30.579392
457.884373	25774.224789	30.584410
458.161872	25830.261658	30.589428
458.874367	25865.812263	30.594445
458.869644	25906.307679	30.599463
459.520531	25940.121163	30.604480
460.128746	25991.129517	30.609498
460.441035	26044.161590	30.614516
461.175064	26090.569369	30.619533
461.372982	26142.538741	30.624551
462.004113	26185.686464	30.629568
462.513587	26225.864115	30.634586
463.079447	26272.505246	30.639604
463.654591	26315.309272	30.644621
463.867043	26363.961679	30.649639
464.509855	26405.726409	30.654656
465.325924	26443.885504	30.659674
465.425265	26486.046340	30.664692
466.169257	26524.107137	30.669709
466.368018	26574.809603	30.674727
466.653778	26609.404027	30.679744
467.103737	26664.027121	30.684762
467.624018	26714.705180	30.689780
468.199686	26755.623864	30.694797
468.781947	26799.020944	30.699815
469.320934	26839.425413	30.704832
469.783360	26882.202180	30.709850
470.014997	26938.079889	30.714868
470.672085	26981.745792	30.719885
470.933097	27025.083041	30.724903
471.598731	27058.363169	30.729920
472.320529	27105.002822	30.734938
472.314661	27151.072182	30.739956
473.261666	27188.605590	30.744973
473.250293	27244.934588	30.749991
473.678945	27290.635887	30.755008
474.444282	27332.054507	30.760026
474.790060	27384.416382	30.765044
475.200863	27423.764571	30.770061
476.038303	27479.493300	30.775079
476.647221	27519.465071	30.780096
477.383801	27559.724957	30.785114
477.507398	27598.553247	30.790132
478.298056	27632.003064	30.795149
478.573295	27687.207195	30.800167
479.103800	27717.659191	30.805184
479.320757	27747.693090	30.810202
479.905585	27801.808485	30.815220
480.102979	27835.432581	30.820237
480.630923	27891.030879	30.825255
481.296597	27927.350589	30.830272
482.010050	27971.356669	30.835290
481.922060	28023.899509	30.840308
482.633430	28059.558919	30.845325
482.650485	28106.380980	30.850343
483.654923	28141.061429	30.855360
483.928122	28185.626728	30.860378
484.159807	28227.082165	30.865396
485.103329	28270.319040	30.870413
485.593073	28299.428586	30.875431
485.578756	28339.921802	30.880448
486.123446	28377.208889	30.885466
486.671693	28421.735585	30.890484
487.101049	28461.152457	30.895501
487.402656	28515.430509	30.900519
487.953676	28559.439719	30.905536
488.555114	28616.889481	30.910554
489.013435	28657.182184	30.915572
489.543292	28708.009594	30.920589
489.738967	28754.008827	30.925607
489.855257	28819.909216	30.930624
490.570022	28868.700037	30.935642
490.745707	28925.489351	30.940660
491.943585	28966.061048	30.945677
492.110611	29030.376416	30.950695
492.338560	29087.902153	30.955712
492.981661	29138.197833	30.960730
493.635098	29201.449021	30.965748
494.119840	29255.440365	30.970765
495.281956	29309.155730	30.975783
495.580953	29360.540643	30.980800
495.952432	29413.999111	30.985818
496.256945	29457.508729	30.990836
497.246074	29511.038806	30.995853
497.620581	29554.000743	31.000871
498.095303	29607.688803	31.005888
498.879798	29656.066450	31.010906
499.191497	29705.961133	31.015924
500.005533	29754.185879	31.020941
500.506497	29795.139847	31.025959
500.807145	29836.846397	31.030976
501.401383	29892.654635	31.035994
501.594056	29944.825520	31.041012
502.207273	29982.751471	31.046029
503.157789	30041.132510	31.051047
503.295893	30084.551330	31.056064
504.130487	30129.473541	31.061082
504.614326	30173.854449	31.066100
505.082916	30214.966196	31.071117
505.455488	30266.644473	31.076135
505.483548	30306.393776	31.081152
506.547334	30364.709822	31.086170
507.169749	30412.226642	31.091188
507.580488	30457.718336	31.096205
508.381261	30499.406801	31.101223
508.565364	30552.268719	31.106240
508.994070	30596.599870	31.111258
509.101652	30648.386219	31.116276
510.002646	30694.740786	31.121293
510.304823	30749.186569	31.126311
510.643887	30796.502058	31.131328
511.375092	30837.953580	31.136346
511.577691	30897.966245	31.141364
512.095790	30942.428612	31.146381
512.782395	30996.792615	31.151399
512.909312	31060.213348	31.156416
513.746437	31110.012447	31.161434
513.880164	31173.028590	31.166452
514.720900	31223.278609	31.171469
515.296035	31271.502879	31.176487
515.646826	31328.883096	31.181504
516.327006	31382.615144	31.186522
516.981121	31422.929126	31.191540
517.464116	31471.207052	31.196557
517.793052	31518.065478	31.201575
518.158989	31564.498251	31.206592
518.651236	31620.505539	31.211610
518.931798	31674.796830	31.216628
519.741706	31716.802197	31.221645
520.305998	31773.170376	31.226663
520.624680	31822.624992	31.231680
521.269704	31872.902935	31.236698
521.710096	31932.674663	31.241716
522.093870	31980.872581	31.246733
522.758302	32041.721452	31.251751
522.871332	32097.581588	31.256768
523.439483	32144.922729	31.261786
523.935177	32218.276595	31.266804
524.883119	32274.043307	31.271821
525.334253	32325.869223	31.276839
525.803150	32388.354600	31.281856
526.848512	32446.336635	31.286874
527.047175	32507.712251	31.291892
527.803143	32559.721913	31.296909
528.429735	32615.590206	31.301927
529.202706	32664.552318	31.306944
530.116757	32702.487981	31.311962
530.081411	32758.381057	31.316980
530.576943	32804.514792	31.321997
531.111947	32853.516801	31.327015
531.426501	32907.503306	31.332032
532.050024	32956.052331	31.337050
532.314239	33021.401172	31.342068
532.870610	33075.771018	31.347085
533.798737	33130.625431	31.352103
534.075918	33204.792641	31.357120
534.645139	33247.696628	31.362138
535.208273	33309.740487	31.367156
535.512667	33358.829380	31.372173
536.173622	33419.598343	31.377191
536.751934	33477.519023	31.382208
537.621384	33531.295685	31.387226
538.276343	33594.448751	31.392244
538.441318	33641.336751	31.397261
539.196943	33698.269485	31.402279
539.536060	33755.517464	31.407296
540.095346	33807.108897	31.412314
540.815709	33864.076396	31.417332
541.332366	33915.829827	31.422349
542.076109	33978.313171	31.427367
542.595372	34033.799738	31.432384
543.216314	34085.526937	31.437402
543.464775	34141.519386	31.442420
544.081313	34191.931672	31.447437
544.688450	34248.436300	31.452455
544.766439	34314.568602	31.457472
545.410623	34356.197380	31.462490
546.051868	34425.629371	31.467508
546.441907	34488.412863	31.472525
547.136970	34537.708593	31.477543
547.647663	34601.728537	31.482560
548.201513	34654.566713	31.487578
548.880195	34720.058309	31.492596
549.104323	34784.953158	31.497613
549.830622	34830.750979	31.502631
550.354650	34897.925650	31.507648
551.191869	34956.199607	31.512666
551.593759	35017.998350	31.517684
552.089305	35079.406254	31.522701
552.522708	35121.283133	31.527719
553.234322	35181.200750	31.532736
554.182928	35219.120273	31.537754
554.777635	35275.330378	31.542772
554.921206	35316.463525	31.547789
555.568074	35368.960192	31.552807
555.862526	35435.095514	31.557824
556.591777	35468.153775	31.562842
556.874269	35529.226060	31.567860
557.552082	35591.296717	31.572877
558.061274	35636.056316	31.577895
558.277800	35700.018384	31.582912
559.125751	35755.689433	31.587930
559.729321	35820.566259	31.592948
559.835824	35871.976596	31.597965
560.367834	35933.346662	31.602983
560.822589	36007.830615	31.608000
561.930242	36067.732995	31.613018
562.490319	36129.922825	31.618036
562.720104	36200.032562	31.623053
563.516923	36252.936225	31.628071
563.651534	36326.527626	31.633088
564.479664	36380.931961	31.638106
564.892456	36454.250610	31.643124
565.338817	36525.323118	31.648141
566.124569	36586.539795	31.653159
566.724534	36661.879835	31.658176
567.407832	36721.942973	31.663194
568.101760	36789.891942	31.668212
568.875868	36854.220328	31.673229
569.352430	36921.931166	31.678247
570.011799	36990.442105	31.683264
570.972114	37044.356283	31.688282
571.382540	37106.574230	31.693300
571.565844	37172.929986	31.698317
572.455418	37224.975260	31.703335
572.775828	37286.056670	31.708352
573.382531	37345.629539	31.713370
573.940281	37411.090941	31.718388
574.447084	37477.144931	31.723405
575.202256	37540.626673	31.728423
575.526454	37613.888914	31.733440
576.170405	37668.378093	31.738458
577.152501	37741.484646	31.743476
577.369062	37803.680242	31.748493
578.067927	37864.218044	31.753511
578.529807	37932.787307	31.758528
579.333629	37997.594603	31.763546
580.065092	38057.692069	31.768564
580.544852	38123.490894	31.773581
580.943488	38187.460006	31.778599
581.740031	38257.237701	31.783616
582.479088	38321.839070	31.788634
583.084646	38381.926872	31.793652
583.369083	38446.689129	31.798669
584.107187	38499.473329	31.803687
584.510570	38563.143102	31.808704
585.083039	38616.602134	31.813722
585.970063	38682.862732	31.818740
586.401876	38752.724765	31.823757
586.829199	38812.278450	31.828775
587.396809	38881.108402	31.833792
588.017862	38943.177819	31.838810
589.035032	38996.362361	31.843828
589.281383	39073.907909	31.848845
590.073068	39126.798694	31.853863
590.481750	39185.343400	31.858880
591.140574	39256.738642	31.863898
591.814370	39306.732713	31.868916
592.212826	39367.183154	31.873933
592.603454	39418.064053	31.878951
593.108143	39484.697012	31.883968
593.716147	39541.142246	31.888986
594.633177	39604.080374	31.894004
594.888260	39668.091038	31.899021
595.587023	39726.984067	31.904039
595.994987	39790.638407	31.909056
596.778981	39847.077561	31.914074
597.173024	39907.356889	31.919092
597.689546	39986.155857	31.924109
598.675592	40045.485361	31.929127
599.013658	40104.694978	31.934144
599.472188	40169.163028	31.939162
600.045030	40233.337747	31.944180
600.569982	40311.533761	31.949197
601.403724	40374.207350	31.954215
602.021247	40441.232339	31.959232
602.602248	40507.133458	31.964250
603.390427	40578.556630	31.969268
604.072734	40639.728252	31.974285
604.871331	40701.616393	31.979303
604.850630	40769.070172	31.984320
605.806221	40838.784022	31.989338
606.352946	40904.335500	31.994356
606.933005	40977.928735	31.999373
607.700274	41049.556076	32.004391
608.144578	41120.103780	32.009408
608.850250	41173.898638	32.014426
609.415287	41246.112672	32.019444
609.614045	41325.443481	32.024461
610.501190	41390.934047	32.029479
611.006093	41469.173006	32.034496
611.570773	41547.219297	32.039514
612.725502	41613.597705	32.044532
612.833259	41696.449483	32.049549
613.506623	41763.877290	32.054567
614.194005	41842.861118	32.059584
614.984761	41905.351275	32.064602
615.405502	41979.161116	32.069620
615.961672	42059.569332	32.074637
616.721270	42133.611021	32.079655
617.117807	42208.268732	32.084672
617.705082	42295.467010	32.089690
618.626271	42365.596419	32.094708
619.078393	42435.225935	32.099725
619.807752	42507.916527	32.104743
620.617643	42584.329062	32.109760
620.935023	42656.081243	32.114778
621.806036	42729.958483	32.119796
622.442082	42810.956606	32.124813
623.145910	42877.562528	32.129831
623.593791	42953.638657	32.134848
623.958380	43027.619807	32.139866
624.695280	43093.400133	32.144884
625.389138	43176.887704	32.149901
626.078544	43252.729338	32.154919
627.092942	43331.444365	32.159936
627.106441	43402.277229	32.164954
628.252709	43472.531434	32.169972
628.945387	43547.113934	32.174989
629.730784	43621.997130	32.180007
630.342877	43675.347418	32.185024
630.854569	43761.639934	32.190042
631.602836	43813.607242	32.195060
632.290546	43877.661885	32.200077
632.684980	43937.812152	32.205095
633.378400	44008.421148	32.210112
633.882710	44072.478384	32.215130
634.573808	44127.736628	32.220148
634.969331	44196.485347	32.225165
635.442480	44271.927999	32.230183
636.345441	44338.638794	32.235200
636.662822	44404.524712	32.240218
637.635311	44463.011738	32.245236
638.241802	44540.255303	32.250253
638.608260	44608.100964	32.255271
639.488524	44675.151411	32.260288
639.637448	44745.265956	32.265306
640.236723	44815.056804	32.270324
641.044609	44898.672112	32.275341
641.357839	44974.541898	32.280359
642.476489	45050.641866	32.285376
642.851638	45129.495464	32.290394
643.409518	45197.229478	32.295412
644.114641	45282.019191	32.300429
644.619741	45362.854225	32.305447
645.499391	45441.925642	32.310464
646.019875	45525.537599	32.315482
646.738034	45599.394598	32.320500
647.286885	45683.870936	32.325517
647.913812	45761.570837	32.330535
648.703772	45836.569463	32.335552
649.028902	45935.394909	32.340570
650.066148	46007.719716	32.345588
650.828457	46097.110838	32.350605
651.311930	46173.948824	32.355623
651.959193	46253.182078	32.360640
652.665043	46342.211073	32.365658
653.603034	46423.519012	32.370676
654.142333	46505.227994	32.375693
654.987759	46582.636169	32.380711
655.730100	46657.838556	32.385728
655.968862	46743.387760	32.390746
656.925317	46816.910082	32.395764
657.673305	46900.212568	32.400781
658.578098	46978.424126	32.405799
659.153901	47049.332382	32.410816
659.622800	47129.413555	32.415834
660.526282	47206.909409	32.420852
660.860648	47282.822835	32.425869
661.577921	47355.887848	32.430887
662.305057	47444.416360	32.435904
662.688034	47527.169320	32.440922
663.787771	47593.915895	32.445940
664.480733	47673.914915	32.450957
665.055232	47757.395124	32.455975
665.799427	47828.581596	32.460992
666.468943	47904.435732	32.466010
667.080205	47970.948629	32.471028
667.984367	48059.962325	32.476045
668.632546	48136.155672	32.481063
669.311179	48204.455219	32.486080
670.119785	48276.652788	32.491098
670.631169	48358.181683	32.496116
671.212818	48418.542591	32.501133
672.029025	48505.801170	32.506151
672.901360	48572.993040	32.511168
673.671691	48652.323288	32.516186
674.498252	48723.114161	32.521204
675.082028	48800.596735	32.526221
675.221846	48880.411226	32.531239
676.312298	48934.316210	32.536256
676.805635	49010.737622	32.541274
677.557611	49075.983556	32.546292
678.229301	49159.823318	32.551309
678.667109	49211.891534	32.556327
679.624917	49278.616939	32.561344
680.071323	49346.949499	32.566362
681.080856	49395.806350	32.571380
681.674567	49464.035998	32.576397
682.205659	49527.447099	32.581415
682.882423	49596.108806	32.586432
683.581406	49670.477455	32.591450
684.269721	49731.409147	32.596468
684.901502	49797.827073	32.601485
685.715465	49866.672344	32.606503
686.178125	49936.649847	32.611520
686.600480	50003.204196	32.616538
686.905927	50083.820626	32.621556
687.602299	50161.533252	32.626573
687.919898	50245.824810	32.631591
689.067361	50325.987105	32.636608
689.749931	50415.664280	32.641626
690.179930	50498.820231	32.646644
691.000754	50572.676311	32.651661
691.592336	50661.314724	32.656679
692.487380	50748.197713	32.661696
693.003609	50842.029473	32.666714
694.048019	50920.429838	32.671732
694.704010	51004.801379	32.676749
695.608906	51090.869354	32.681767
696.291217	51160.018968	32.686784
697.056303	51257.399779	32.691802
697.577674	51338.983843	32.696820
698.633664	51415.249036	32.701837
698.815282	51498.191349	32.706855
700.057504	51579.903551	32.711872
700.668022	51666.793501	32.716890
700.974866	51753.342393	32.721908
701.902962	51838.405364	32.726925
702.381478	51918.526972	32.731943
703.098373	52001.742975	32.736960
704.088317	52086.746260	32.741978
704.650782	52177.967658	32.746996
705.563302	52255.934046	32.752013
706.085006	52350.662959	32.757031
706.605152	52432.870936	32.762048
707.307126	52527.362401	32.767066
708.135824	52605.432499	32.772084
708.881721	52696.607021	32.777101
709.507750	52795.263118	32.782119
710.437143	52873.797783	32.787136
710.938302	52976.954791	32.792154
712.040828	53057.596990	32.797172
712.534298	53144.721367	32.802189
713.064934	53228.036582	32.807207
714.327174	53296.718760	32.812224
714.918681	53389.773210	32.817242
715.501180	53477.434002	32.822260
716.134897	53568.485822	32.827277
716.915854	53652.216327	32.832295
717.720709	53723.913570	32.837312
718.246838	53825.611425	32.842330
719.122806	53904.500235	32.847348
720.481446	53977.016607	32.852365
721.431390	54062.610042	32.857383
721.795492	54130.502301	32.862400
722.415393	54210.515115	32.867418
723.140939	54288.451019	32.872436
723.892757	54363.722878	32.877453
724.586150	54455.331257	32.882471
725.621940	54520.542184	32.887488
726.394631	54596.702368	32.892506
726.618670	54670.975945	32.897524
727.748280	54731.079416	32.902541
727.660093	54805.727389	32.907559
728.303907	54876.438197	32.912576
729.067306	54963.974580	32.917594
729.550284	55039.710509	32.922612
730.563149	55114.095364	32.927629
730.738565	55210.026350	32.932647
731.489507	55288.442208	32.937664
731.841835	55386.859586	32.942682
732.816248	55470.862782	32.947700
733.615566	55559.400520	32.952717
734.202532	55660.573300	32.957735
735.476146	55750.859544	32.962752
735.839195	55848.576055	32.967770
736.647627	55947.179830	32.972788
737.427930	56027.419887	32.977805
738.001550	56130.587699	32.982823
738.928543	56219.423202	32.987840
739.531406	56314.151405	32.992858
740.221326	56411.292135	32.997876
740.834931	56510.404849	33.002893
741.715938	56612.911368	33.007911
742.855167	56706.952404	33.012928
743.472119	56801.491019	33.017946
744.244399	56896.181322	33.022964
745.277769	56991.031097	33.027981
745.786701	57088.198741	33.032999
746.569327	57175.716401	33.038016
747.470120	57279.512183	33.043034
748.233911	57372.847513	33.048052
748.957172	57458.436216	33.053069
749.872967	57546.407415	33.058087
750.496340	57633.182461	33.063104
751.276430	57726.339799	33.068122
752.261634	57827.640946	33.073140
752.921770	57910.120234	33.078157
753.661825	58004.719998	33.083175
754.317984	58103.801962	33.088192
755.075410	58190.342379	33.093210
755.692145	58286.246727	33.098228
756.655910	58382.770323	33.103245
757.373865	58487.986587	33.108263
758.246851	58573.334087	33.113280
759.026348	58672.253096	33.118298
759.622524	58772.915552	33.123316
760.601909	58857.178625	33.128333
761.313265	58950.327722	33.133351
762.160748	59042.968107	33.138368
763.084344	59137.972576	33.143386
763.578523	59220.282446	33.148404
764.424401	59315.534440	33.153421
764.980467	59416.320493	33.158439
765.960513	59512.922641	33.163456
766.577186	59598.582310	33.168474
767.286786	59695.236383	33.173492
768.114009	59781.317036	33.178509
768.890669	59895.341015	33.183527
769.536335	59987.368140	33.188544
770.120049	60081.358843	33.193562
770.966449	60185.001620	33.198580
771.805173	60272.902655	33.203597
772.339986	60381.274896	33.208615
773.587510	60481.623213	33.213632
774.337337	60589.752431	33.218650
774.866333	60685.657377	33.223668
776.010497	60772.113261	33.228685
776.621837	60871.841897	33.233703
777.623893	60954.902754	33.238720
778.352613	61040.120176	33.243738
778.915651	61117.294173	33.248756
780.009498	61194.045675	33.253773
780.727535	61284.417054	33.258791
781.101585	61379.737804	33.263808
782.154585	61464.277627	33.268826
782.304691	61549.352702	33.273844
783.347280	61644.235431	33.278861
784.130887	61738.567301	33.283879
785.196366	61840.741152	33.288896
786.003001	61928.698873	33.293914
786.444853	62019.150782	33.298932
787.154274	62116.859279	33.303949
788.000223	62205.317343	33.308967
788.965538	62316.776375	33.313984
789.582514	62408.528398	33.319002
790.359350	62514.128668	33.324020
791.112383	62613.203937	33.329037
791.790584	62714.371644	33.334055
792.782050	62815.709265	33.339072
793.842393	62913.426712	33.344090
794.329735	63019.545210	33.349108
795.123290	63106.896998	33.354125
795.876692	63221.303656	33.359143
796.507816	63324.972649	33.364160
797.437661	63417.872105	33.369178
798.156360	63531.388619	33.374196
799.335845	63629.608087	33.379213
800.007958	63739.416584	33.384231
801.098691	63843.050080	33.389248
801.899447	63931.877018	33.394266
802.335031	64045.032293	33.399284
803.346180	64140.835679	33.404301
803.985837	64253.724447	33.409319
805.019398	64370.676565	33.414336
805.758979	64458.536057	33.419354
806.301725	64576.702058	33.424372
807.025596	64669.957270	33.429389
808.368778	64784.666941	33.434407
808.926446	64894.652193	33.439424
809.505504	64999.779487	33.444442
810.538327	65110.060260	33.449460
811.789820	65219.116972	33.454477
812.470751	65332.788653	33.459495
813.250149	65435.008623	33.464512
814.070899	65529.035552	33.469530
814.674777	65639.029727	33.474548
815.670054	65749.553996	33.479565
816.348847	65848.233429	33.484583
817.449672	65949.568263	33.489600
818.522922	66050.250668	33.494618
818.759960	66153.594330	33.499636
819.812020	66261.570480	33.504653
820.955834	66364.916930	33.509671
821.609801	66478.504460	33.514688
822.487131	66572.242222	33.519706
822.994609	66686.120631	33.524724
824.068068	66780.939577	33.529741
824.761855	66882.105998	33.534759
825.320599	66988.795567	33.539776
826.553219	67107.089344	33.544794
826.928436	67217.806090	33.549812
827.929826	67314.706748	33.554829
828.614024	67424.342935	33.559847
829.170669	67537.920663	33.564864
830.082807	67640.812229	33.569882
830.817402	67755.474437	33.574900
831.598633	67860.829190	33.579917
832.762825	67965.469908	33.584935
833.400785	68068.952642	33.589952
834.238202	68161.117109	33.594970
834.817719	68268.745442	33.599988
835.810377	68377.033091	33.605005
836.774539	68473.243403	33.610023
837.386828	68589.858766	33.615040
838.306566	68697.009378	33.620058
838.886129	68806.834416	33.625076
839.853522	68924.448781	33.630093
840.561856	69026.754825	33.635111
841.563109	69143.700905	33.640128
842.399223	69252.967337	33.645146
842.882844	69385.320722	33.650164
844.136583	69493.937606	33.655181
844.903313	69604.228986	33.660199
845.470638	69716.779621	33.665216
846.412650	69833.347252	33.670234
847.294685	69953.333586	33.675252
848.389290	70062.826978	33.680269
848.986482	70190.057472	33.685287
850.026306	70300.711957	33.690304
850.969823	70421.291448	33.695322
851.583263	70541.540489	33.700340
852.630057	70666.973197	33.705357
853.931477	70783.726839	33.710375
854.140496	70903.513633	33.715392
855.202818	71020.984710	33.720410
855.705708	71144.556227	33.725428
856.655644	71270.362585	33.730445
857.576015	71401.884708	33.735463
858.285160	71525.519147	33.740480
859.057638	71654.607406	33.745498
859.857015	71780.915912	33.750516
860.718252	71908.985552	33.755533
862.036257	72035.962288	33.760551
862.507172	72176.296500	33.765568
863.860026	72297.115999	33.770586
864.363021	72431.951192	33.775604
865.550268	72566.604492	33.780621
866.201957	72677.860248	33.785639
867.228593	72812.042045	33.790656
868.273885	72934.149127	33.795674
868.997146	73064.031764	33.800692
869.820166	73192.570628	33.805709
870.942366	73312.972271	33.810727
871.689473	73439.267449	33.815744
872.577867	73561.543127	33.820762
873.581621	73697.296228	33.825780
874.355270	73826.656489	33.830797
875.462453	73951.838933	33.835815
876.400076	74086.719993	33.840832
877.306586	74205.302884	33.845850
878.055128	74335.562036	33.850868
878.909588	74458.360614	33.855885
880.028156	74578.839399	33.860903
880.503689	74708.747478	33.865920
881.143218	74828.275967	33.870938
882.397408	74956.235270	33.875956
883.110741	75083.962213	33.880973
884.327041	75209.108486	33.885991
885.011695	75336.240796	33.891008
885.741021	75470.039007	33.896026
886.489231	75597.984524	33.901044
887.299069	75722.770854	33.906061
888.648761	75849.675963	33.911079
889.042706	75992.045995	33.916096
890.168051	76102.051718	33.921114
890.819492	76232.439339	33.926132
891.771607	76348.395058	33.931149
892.786398	76470.027180	33.936167
893.295731	76594.298870	33.941184
894.346213	76704.010036	33.946202
895.463844	76831.692858	33.951220
896.066816	76956.235715	33.956237
897.245133	77077.717618	33.961255
897.954975	77208.600997	33.966272
898.777883	77326.019006	33.971290
899.808891	77454.719114	33.976308
900.824893	77600.076970	33.981325
901.681245	77720.527671	33.986343
902.177364	77852.531806	33.991360
903.026500	77982.005099	33.996378
903.852350	78125.936651	34.001396
904.667611	78264.285467	34.006413
905.781242	78401.510453	34.011431
906.542077	78539.648575	34.016448
907.493324	78680.950490	34.021466
908.244763	78816.833628	34.026484
908.995880	78962.826090	34.031501
910.144161	79104.490274	34.036519
910.878336	79254.213282	34.041536
912.152379	79393.492647	34.046554
913.052072	79542.127457	34.051572
914.024971	79687.385763	34.056589
915.060238	79824.056725	34.061607
915.703763	79973.502174	34.066624
916.878915	80108.987745	34.071642
917.670579	80262.686987	34.076660
918.455012	80405.874496	34.081677
920.029458	80558.389831	34.086695
920.685979	80705.807266	34.091712
921.720267	80837.461517	34.096730
922.681909	80980.471513	34.101748
923.319717	81123.086794	34.106765
924.762423	81265.810258	34.111783
925.534789	81408.588537	34.116800
926.636723	81544.860268	34.121818
927.975393	81681.144275	34.126836
928.821648	81822.261717	34.131853
929.776998	81955.801793	34.136871
930.515215	82103.240053	34.141888
931.625180	82225.956694	34.146906
932.657695	82359.771061	34.151924
933.240993	82502.182524	34.156941
934.461811	82624.781740	34.161959
935.132524	82781.092909	34.166976
936.089310	82906.267991	34.171994
937.168563	83050.897457	34.177012
938.136170	83192.155097	34.182029
938.696163	83329.760792	34.187047
939.831604	83464.298483	34.192064
940.703113	83611.256170	34.197082
941.797829	83741.563136	34.202100
942.535298	83898.244127	34.207117
943.616554	84033.578647	34.212135
944.399376	84178.137651	34.217152
945.085993	84320.682443	34.222170
946.294072	84461.047569	34.227188
946.956851	84614.158218	34.232205
947.752707	84751.018369	34.237223
948.706156	84905.898802	34.242240
950.015475	85050.002849	34.247258
951.059398	85194.537647	34.252276
951.671263	85337.784390	34.257293
952.705232	85469.686630	34.262311
953.938788	85613.060042	34.267328
954.631497	85731.295801	34.272346
955.695667	85872.294343	34.277364
956.985686	86009.985002	34.282381
957.798684	86137.466571	34.287399
958.413019	86262.267103	34.292416
959.432306	86395.967729	34.297434
960.586541	86541.783463	34.302452
961.053984	86689.023532	34.307469
962.427972	86823.876547	34.312487
962.896685	86970.485380	34.317504
963.876202	87107.980705	34.322522
965.402902	87244.740894	34.327540
965.652756	87393.691924	34.332557
966.664531	87537.968035	34.337575
967.644429	87696.165745	34.342592
968.764364	87853.809792	34.347610
969.675897	87998.023019	34.352628
970.069021	88147.379080	34.357645
971.306465	88306.481175	34.362663
972.707622	88469.006180	34.367680
973.469527	88622.253093	34.372698
974.832867	88766.276032	34.377716
975.611183	88930.666470	34.382733
976.654018	89087.223974	34.387751
977.739832	89231.339914	34.392768
978.323802	89389.051119	34.397786
979.626322	89549.138000	34.402804
980.357938	89709.535530	34.407821
981.302050	89864.057644	34.412839
982.441875	90024.510024	34.417856
983.205640	90188.645701	34.422874
984.081174	90351.624836	34.427892
984.997333	90519.838626	34.432909
985.769068	90683.463724	34.437927
986.805037	90857.830711	34.442944
987.785277	91028.543705	34.447962
989.293308	91191.791008	34.452980
989.988232	91374.509117	34.457997
991.189566	91533.581637	34.463015
992.178203	91707.089159	34.468032
993.172271	91876.869136	34.473050
994.388733	92033.581648	34.478068
995.501501	92203.837961	34.483085
996.186826	92363.387330	34.488103
997.595462	92529.527251	34.493120
998.777537	92695.344994	34.498138
999.543748	92857.833721	34.503156
1000.747236	93028.511194	34.508173
1001.854341	93184.090893	34.513191
1002.516959	93350.752191	34.518208
1003.777611	93514.948460	34.523226
1004.752425	93671.129121	34.528244
1005.696265	93844.583293	34.533261
1006.603208	94002.435662	34.538279
1007.898068	94169.934775	34.543296
1008.785426	94327.817789	34.548314
1009.875191	94478.813111	34.553332
1010.353976	94655.394552	34.558349
1011.574952	94822.479881	34.563367
1012.633079	94979.750141	34.568384
1013.535951	95150.732588	34.573402
1014.818369	95316.810951	34.578420
1015.454126	95492.916642	34.583437
1016.653741	95657.232214	34.588455
1017.686105	95821.361301	34.593472
1018.598574	95985.707533	34.598490
1020.400987	96142.792461	34.603508
1020.991014	96296.255337	34.608525
1021.719618	96444.625627	34.613543
1023.324733	96585.337690	34.618560
1024.218089	96736.600782	34.623578
1025.117865	96877.905904	34.628596
1025.856987	97035.628059	34.633613
1026.907028	97195.844675	34.638631
1028.020178	97356.355747	34.643648
1028.769092	97516.826781	34.648666
1029.874477	97670.200196	34.653684
1030.759640	97841.957345	34.658701
1031.420575	97998.470311	34.663719
1032.726258	98166.418666	34.668736
1033.635692	98337.915616	34.673754
1034.648980	98503.223954	34.678772
1035.866236	98680.901912	34.683789
1036.572926	98847.915565	34.688807
1037.759573	99014.338147	34.693824
1038.327584	99200.389052	34.698842
1039.980027	99369.098422	34.703860
1040.667049	99558.646024	34.708877
1042.133195	99736.283880	34.713895
1043.240308	99902.427857	34.718912
1043.914527	100085.897190	34.723930
1045.196915	100252.660252	34.728948
1046.561992	100445.964425	34.733965
1047.657309	100608.860625	34.738983
1048.374625	100782.881382	34.744000
1049.769416	100961.843825	34.749018
1050.592788	101135.184627	34.754036
1051.768065	101313.312060	34.759053
1052.691897	101481.782271	34.764071
1054.030003	101660.638644	34.769088
1054.938108	101848.710329	34.774106
1056.056474	102016.157783	34.779124
1057.143595	102206.817482	34.784141
1058.107552	102384.240088	34.789159
1059.576998	102558.180113	34.794176
1060.137498	102749.418425	34.799194
1061.637846	102913.541245	34.804212
1062.507989	103092.396224	34.809229
1063.372283	103275.147607	34.814247
1064.750199	103451.901172	34.819264
1065.774956	103638.098550	34.824282
1067.479490	103803.010054	34.829300
1068.521799	103982.292244	34.834317
1069.460951	104149.130826	34.839335
1070.311849	104321.684132	34.844352
1071.242055	104506.586192	34.849370
1072.733808	104680.770958	34.854388
1073.369310	104847.486870	34.859405
1074.273630	105025.279205	34.864423
1075.492525	105211.962234	34.869440
1076.357070	105391.004779	34.874458
1077.876625	105566.697945	34.879476
1078.799348	105752.103909	34.884493
1079.725337	105939.549753	34.889511
1081.062923	106110.261120	34.894528
1082.233997	106302.988500	34.899546
1083.361513	106473.812926	34.904564
1084.562216	106654.404278	34.909581
1085.337501	106826.631767	34.914599
1086.528206	107005.631258	34.919616
1087.564918	107190.154438	34.924634
1088.597347	107362.165536	34.929652
1089.718094	107535.619741	34.934669
1090.780552	107715.582473	34.939687
1092.045689	107888.001784	34.944704
1092.816019	108060.820669	34.949722
1094.203711	108221.492789	34.954740
1095.262547	108388.781502	34.959757
1096.070227	108554.212785	34.964775
1097.595799	108712.749711	34.969792
1098.413400	108901.994860	34.974810
1099.573175	109056.781582	34.979828
1100.570039	109233.231227	34.984845
1101.392511	109409.026834	34.989863
1102.721955	109577.367511	34.994880
1103.315576	109749.187685	34.999898
1104.223378	109925.441204	35.004916
1105.769376	110111.078181	35.009933
1106.446043	110304.384598	35.014951
1107.861266	110485.067439	35.019968
1109.002504	110671.421183	35.024986
1109.948278	110857.909852	35.030004
1111.528167	111044.193607	35.035021
1112.371910	111233.906642	35.040039
1113.893953	111412.082360	35.045056
1114.916323	111600.020210	35.050074
1115.956050	111788.146491	35.055092
1117.175345	111982.933173	35.060109
1118.259123	112168.926505	35.065127
1119.428353	112349.978963	35.070144
1120.439531	112534.795927	35.075162
1121.220841	112726.037065	35.080180
1122.647664	112923.937843	35.085197
1123.419463	113118.857155	35.090215
1125.134777	113308.858370	35.095232
1126.069958	113506.261798	35.100250
1127.076922	113698.017057	35.105268
1128.399357	113896.423408	35.110285
1129.317763	114095.126006	35.115303
1130.689488	114280.743750	35.120320
1132.058047	114479.121257	35.125338
1133.317650	114669.207038	35.130356
1134.308265	114863.101412	35.135373
1135.362500	115046.952288	35.140391
1136.682335	115241.947768	35.145408
1137.501614	115426.752172	35.150426
1138.829877	115635.166239	35.155444
1139.925828	115819.331978	35.160461
1140.967153	116022.563645	35.165479
1142.191160	116216.225970	35.170496
1143.590502	116422.771553	35.175514
1144.640504	116602.223967	35.180532
1145.921814	116799.225729	35.185549
1146.899673	116999.180548	35.190567
1148.381461	117179.097356	35.195584
1149.397106	117389.552522	35.200602
1150.581220	117581.254064	35.205620
1151.708498	117773.219694	35.210637
1152.735286	117966.989810	35.215655
1154.053514	118149.892045	35.220672
1155.159616	118353.839097	35.225690
1156.355270	118548.750934	35.230708
1157.934889	118732.335894	35.235725
1158.764617	118931.669696	35.240743
1160.597517	119110.564810	35.245760
1161.561872	119302.402786	35.250778
1162.471990	119496.012335	35.255796
1163.636405	119679.760617	35.260813
1164.813601	119861.974666	35.265831
1165.969484	120049.046666	35.270848
1166.935800	120244.387914	35.275866
1167.993049	120424.192290	35.280884
1169.288922	120607.785270	35.285901
1170.087669	120787.229096	35.290919
1171.591600	120965.885811	35.295936
1172.722575	121152.094570	35.300954
1173.641635	121326.085386	35.305972
1175.004246	121509.761656	35.310989
1175.739215	121697.521986	35.316007
1177.123358	121880.385955	35.321024
1178.498490	122064.241007	35.326042
1179.238829	122244.856536	35.331060
1180.654062	122443.027484	35.336077
1181.718231	122635.935170	35.341095
1182.877705	122809.742854	35.346112
1184.006268	123014.668986	35.351130
1185.087611	123215.624961	35.356148
1186.249399	123399.853009	35.361165
1187.425694	123609.312325	35.366183
1188.535848	123800.686436	35.371200
1190.130985	124003.894649	35.376218
1191.303039	124198.074561	35.381236
1192.740372	124395.684443	35.386253
1193.322285	124590.255924	35.391271
1194.650366	124800.116643	35.396288
1196.141344	125007.924063	35.401306
1197.412417	125211.244647	35.406324
1198.546428	125404.716158	35.411341
1199.507362	125615.530380	35.416359
1201.182299	125818.737558	35.421376
1202.090135	126022.453124	35.426394
1203.612765	126230.821313	35.431412
1204.978867	126423.031483	35.436429
1206.020846	126640.277993	35.441447
1207.667388	126829.060236	35.446464
1208.590956	127032.843272	35.451482
1209.787805	127234.072866	35.456500
1211.212384	127439.157317	35.461517
1212.347397	127637.535232	35.466535
1213.255389	127840.641713	35.471552
1214.123682	128052.286454	35.476570
1215.418656	128264.508538	35.481588
1216.914904	128465.050184	35.486605
1218.049668	128673.346837	35.491623
1219.400861	128881.685155	35.496640
1220.494694	129093.984150	35.501658
1221.487063	129307.492865	35.506676
1223.328349	129519.709210	35.511693
1224.168344	129734.906537	35.516711
1225.401920	129943.626262	35.521728
1226.726924	130158.911093	35.526746
1227.667403	130374.273628	35.531764
1229.047975	130584.557794	35.536781
1230.256097	130812.238322	35.541799
1231.297617	131013.200945	35.546816
1232.805236	131239.149069	35.551834
1233.812002	131445.266789	35.556852
1235.095887	131664.599743	35.561869
1236.092936	131888.595925	35.566887
1237.727681	132109.243007	35.571904
1238.987538	132326.974514	35.576922
1239.998818	132553.216780	35.581940
1241.358184	132769.553044	35.586957
1242.452984	132989.154476	35.591975
1243.732793	133210.843909	35.596992
1245.120496	133434.241135	35.602010
1246.215562	133654.125929	35.607028
1247.913478	133872.530716	35.612045
1248.918271	134089.910561	35.617063
1250.077001	134294.639496	35.622080
1251.278960	134489.689483	35.627098
1252.604414	134700.073004	35.632116
1254.015769	134903.901901	35.637133
1254.752869	135118.137999	35.642151
1255.965417	135315.270324	35.647168
1257.310315	135516.172699	35.652186
1258.352647	135740.935920	35.657204
1259.515734	135950.821785	35.662221
1260.569659	136175.471934	35.667239
1262.046857	136395.210478	35.672256
1263.224966	136610.486362	35.677274
1264.353577	136848.415791	35.682292
1265.518376	137062.847328	35.687309
1266.760243	137291.822724	35.692327
1268.214460	137517.645586	35.697344
1269.656407	137743.611465	35.702362
1270.553576	137977.732769	35.707380
1271.967248	138204.733417	35.712397
1273.068823	138444.542452	35.717415
1274.532989	138683.976271	35.722432
1275.917913	138915.081849	35.727450
1276.874760	139147.426267	35.732468
1278.471377	139381.150030	35.737485
1279.640981	139630.960361	35.742503
1281.130564	139863.627350	35.747520
1282.622821	140097.487382	35.752538
1283.893721	140337.953785	35.757556
1285.268383	140566.269968	35.762573
1286.525306	140809.316013	35.767591
1287.803489	141039.604009	35.772608
1289.245399	141275.876914	35.777626
1290.606213	141517.782223	35.782644
1291.974282	141743.495119	35.787661
1293.098615	141990.984151	35.792679
1294.450645	142229.066343	35.797696
1296.184884	142456.245002	35.802714
1297.171650	142689.331110	35.807732
1298.608482	142936.813224	35.812749
1300.216160	143176.787089	35.817767
1301.476586	143408.298337	35.822784
1302.650627	143637.859811	35.827802
1303.832540	143877.274755	35.832820
1305.403371	144105.771865	35.837837
1306.604019	144347.761184	35.842855
1307.851696	144582.287687	35.847872
1309.557037	144815.332440	35.852890
1310.377658	145059.557940	35.857908
1311.844033	145290.590864	35.862925
1313.162761	145531.680963	35.867943
1314.603785	145774.819608	35.872960
1316.439122	145995.536456	35.877978
1317.608541	146248.513641	35.882996
1318.685200	146468.534440	35.888013
1320.198489	146716.093525	35.893031
1321.197940	146946.846434	35.898048
1322.667574	147172.221870	35.903066
1324.324803	147414.156312	35.908084
1325.467413	147650.812705	35.913101
1327.234221	147883.740237	35.918119
1328.149209	148120.031433	35.923136
1329.474603	148344.981344	35.928154
1330.644100	148585.228525	35.933172
1331.843320	148809.377733	35.938189
1333.179481	149053.976015	35.943207
1334.721436	149293.037439	35.948224
1336.021847	149524.517742	35.953242
1337.036252	149768.615839	35.958260
1338.779779	149992.758314	35.963277
1339.891196	150209.206318	35.968295
1341.062230	150426.165739	35.973312
1342.656292	150645.935659	35.978330
1343.603659	150874.819106	35.983348
1344.917876	151102.856920	35.988365
1346.368431	151328.818805	35.993383
1347.285833	151558.510415	35.998400
1348.635344	151782.817435	36.003418
1349.893485	152018.594521	36.008436
1351.238579	152261.119304	36.013453
1352.351030	152496.555579	36.018471
1353.643185	152745.687938	36.023488
1355.272180	152975.689034	36.028506
1356.334469	153232.016483	36.033524
1357.681535	153480.040972	36.038541
1359.042085	153726.618783	36.043559
1360.149698	153987.357966	36.048576
1361.607881	154237.144779	36.053594
1363.232852	154490.330525	36.058612
1364.572759	154751.391599	36.063629
1366.209407	155003.005806	36.068647
1367.571680	155265.335100	36.073664
1368.771701	155515.857723	36.078682
1370.171989	155792.023722	36.083700
1371.578622	156032.278497	36.088717
1373.666862	156285.399223	36.093735
1374.528200	156546.310233	36.098752
1376.300899	156792.331729	36.103770
1377.907774	157054.378716	36.108788
1379.281429	157308.309049	36.113805
1380.745514	157551.493870	36.118823
1382.243837	157808.159570	36.123840
1383.858291	158046.324295	36.128858
1385.224565	158309.916154	36.133876
1386.466937	158554.158528	36.138893
1387.981952	158804.066088	36.143911
1389.103131	159048.534433	36.148928
1390.707091	159303.758577	36.153946
1392.028432	159551.787078	36.158964
1393.312122	159811.393371	36.163981
1394.779197	160059.502340	36.168999
1395.898073	160321.245046	36.174016
1397.664182	160573.139043	36.179034
1398.748391	160833.431737	36.184052
1400.058165	161090.339445	36.189069
1401.529202	161348.985570	36.194087
1402.977788	161612.978245	36.199104
1404.726016	161863.639655	36.204122
1406.224552	162122.527058	36.209140
1407.175702	162379.489234	36.214157
1408.709318	162642.814569	36.219175
1409.959874	162907.799619	36.224192
1411.721245	163164.353528	36.229210
1412.917869	163426.013901	36.234228
1414.085436	163686.944792	36.239245
1415.829584	163943.747288	36.244263
1417.036408	164223.363977	36.249280
1418.790611	164473.786003	36.254298
1419.858840	164741.299331	36.259316
1421.372768	165008.854846	36.264333
1423.177418	165271.301404	36.269351
1424.426803	165535.198938	36.274368
1425.837590	165787.601196	36.279386
1427.337127	166054.467638	36.284404
1428.371761	166317.796325	36.289421
1429.876300	166576.963234	36.294439
1431.161918	166850.163331	36.299456
1432.901137	167097.456067	36.304474
1434.331732	167361.892877	36.309492
1435.753744	167599.242109	36.314509
1437.276845	167843.504008	36.319527
1438.352418	168098.537955	36.324544
1440.094813	168334.594618	36.329562
1441.357829	168590.285578	36.334580
1442.411199	168844.439174	36.339597
1444.169338	169085.052552	36.344615
1445.595725	169345.783763	36.349632
1446.745446	169613.744354	36.354650
1448.397094	169871.675063	36.359668
1449.550541	170128.839353	36.364685
1451.284382	170390.959616	36.369703
1452.494684	170650.452299	36.374720
1453.997886	170924.364300	36.379738
1455.376467	171189.377593	36.384756
1456.827136	171458.631581	36.389773
1458.348496	171723.268995	36.394791
1459.546093	172000.537192	36.399808
1460.950598	172275.920081	36.404826
1462.743289	172547.128823	36.409844
1463.918341	172821.867541	36.414861
1465.811003	173103.151670	36.419879
1467.153478	173385.251728	36.424896
1468.416081	173654.917322	36.429914
1470.052189	173943.076247	36.434932
1471.082833	174219.750435	36.439949
1473.234033	174497.459348	36.444967
1474.380918	174795.590228	36.449984
1475.623323	175075.813100	36.455002
1477.324149	175355.213068	36.460020
1478.723556	175663.231796	36.465037
1480.582587	175944.982194	36.470055
1481.469606	176238.900612	36.475072
1483.523324	176527.272306	36.480090
1484.997606	176819.358433	36.485108
1486.621041	177114.619842	36.490125
1488.093264	177404.285686	36.495143
1489.438633	177695.268693	36.500160
1491.237946	177984.071574	36.505178
1492.647188	178272.090221	36.510196
1493.893303	178568.729739	36.515213
1495.758259	178854.138042	36.520231
1496.832528	179169.009451	36.525248
1498.343322	179457.893748	36.530266
1499.659408	179752.700924	36.535284
1500.985023	180055.808819	36.540301
1503.064531	180368.528789	36.545319
1504.407940	180667.080826	36.550336
1505.751416	180973.313393	36.555354
1507.563676	181275.941808	36.560372
1508.657374	181584.237287	36.565389
1510.430563	181878.803221	36.570407
1511.824637	182184.945603	36.575424
1513.125137	182502.312818	36.580442
1514.883201	182805.923544	36.585460
1516.218514	183120.775503	36.590477
1517.759261	183424.590628	36.595495
1519.067335	183743.436272	36.600512
1520.654536	184056.982749	36.605530
1522.032491	184386.698523	36.610548
1523.441482	184705.203076	36.615565
1525.119406	185021.964136	36.620583
1526.278240	185334.662062	36.625600
1527.878396	185653.597437	36.630618
1529.791236	185971.924457	36.635636
1531.002318	186295.928999	36.640653
1532.820440	186605.922912	36.645671
1534.565564	186909.114081	36.650688
1535.708464	187207.303489	36.655706
1537.512237	187495.890295	36.660724
1538.902002	187812.993917	36.665741
1540.613743	188100.329578	36.670759
1541.747674	188397.143000	36.675776
1543.161725	188697.884898	36.680794
1544.991582	188999.257820	36.685812
1546.069694	189317.068544	36.690829
1547.647983	189627.321418	36.695847
1549.552719	189946.293767	36.700864
1550.602712	190246.227816	36.705882
1552.025602	190574.600832	36.710900
1553.564164	190902.106000	36.715917
1555.156903	191212.009277	36.720935
1556.721840	191539.386598	36.725952
1558.324942	191872.078470	36.730970
1560.213321	192191.954044	36.735988
1561.690412	192530.027517	36.741005
1563.408805	192856.650218	36.746023
1564.546708	193183.713314	36.751040
1566.363556	193516.734195	36.756058
1568.235259	193850.611052	36.761076
1569.633421	194185.304239	36.766093
1571.323324	194508.753761	36.771111
1572.957267	194848.794287	36.776128
1574.169522	195182.203115	36.781146
1576.019825	195516.815886	36.786164
1577.327881	195863.237963	36.791181
1579.175612	196192.979561	36.796199
1580.622170	196535.941819	36.801216
1582.619133	196870.727746	36.806234
1584.188767	197205.370142	36.811252
1585.667978	197555.581598	36.816269
1587.611617	197900.779440	36.821287
1589.068892	198232.906358	36.826304
1590.574339	198573.660269	36.831322
1592.465586	198900.551465	36.836340
1593.991622	199249.697489	36.841357
1595.785847	199582.575174	36.846375
1597.356436	199924.683537	36.851392
1598.978351	200264.715594	36.856410
1600.425954	200601.375459	36.861428
1601.822504	200945.561693	36.866445
1604.159850	201279.043334	36.871463
1605.535187	201630.460732	36.876480
1607.167238	201977.749112	36.881498
1608.904171	202302.320076	36.886516
1610.308808	202657.800596	36.891533
1612.248529	202990.606744	36.896551
1613.729256	203323.502929	36.901568
1615.190703	203665.494829	36.906586
1616.936467	204002.908492	36.911604
1618.180753	204357.547592	36.916621
1620.038371	204689.562302	36.921639
1621.607934	205033.294783	36.926656
1623.205375	205381.252395	36.931674
1625.104246	205718.267493	36.936692
1626.438215	206070.284100	36.941709
1628.174721	206419.480458	36.946727
1629.418207	206770.181942	36.951744
1630.990210	207114.862871	36.956762
1632.849146	207467.992587	36.961780
1634.167798	207817.797455	36.966797
1635.913613	208172.752033	36.971815
1637.681421	208518.282795	36.976832
1639.164179	208876.521835	36.981850
1641.078352	209218.602967	36.986868
1642.376860	209553.308149	36.991885
1643.957408	209891.421931	36.996903
1645.755980	210226.351950	37.001920
1646.914006	210564.004920	37.006938
1648.913867	210888.644265	37.011956
1650.388870	211235.009230	37.016973
1651.962861	211567.315002	37.021991
1653.714591	211913.357608	37.027008
1655.103643	212260.756726	37.032026
1657.018546	212613.556041	37.037044
1658.412206	212959.103178	37.042061
1659.873862	213313.656332	37.047079
1661.768055	213668.114028	37.052096
1662.838534	214027.509242	37.057114
1664.768448	214389.862353	37.062132
1666.224960	214759.888895	37.067149
1667.936415	215118.649123	37.072167
1669.719280	215491.723136	37.077184
1670.904700	215864.795722	37.082202
1672.506337	216248.620445	37.087220
1674.020082	216629.210291	37.092237
1675.765712	217008.391831	37.097255
1677.549772	217401.232631	37.102272
1678.879729	217798.137511	37.107290
1680.760098	218175.878964	37.112308
1682.382584	218588.104571	37.117325
1684.093830	218964.987955	37.122343
1686.011691	219384.025544	37.127360
1687.529158	219775.598843	37.132378
1689.715219	220166.199598	37.137396
1691.322137	220574.600434	37.142413
1693.071361	220969.492491	37.147431
1694.790110	221369.089836	37.152448
1696.103961	221777.696003	37.157466
1698.490464	222168.118459	37.162484
1700.228386	222578.333855	37.167501
1701.656792	222964.650258	37.172519
1703.394651	223442.786698	37.177536
1705.100013	223851.437255	37.182554
1707.096211	224257.729822	37.187572
1708.785707	224655.133734	37.192589
1710.603106	225056.505603	37.197607
1712.834091	225457.556477	37.202624
1714.199987	225858.624556	37.207642
1715.994664	226244.687861	37.212660
1717.808671	226657.038297	37.217677
1719.532725	227058.152623	37.222695
1721.471400	227458.572332	37.227712
1722.610237	227862.986240	37.232730
1724.462742	228265.911868	37.237748
1726.515185	228670.532911	37.242765
1728.163024	229066.534982	37.247783
1730.175230	229464.027440	37.252800
1731.997073	229869.426702	37.257818
1733.693978	230270.707423	37.262836
1735.574835	230673.381325	37.267853
1736.836775	231074.964723	37.272871
1739.193235	231459.425932	37.277888
1740.850018	231864.857990	37.282906
1742.389741	232258.879938	37.287924
1744.204517	232662.332109	37.292941
1745.631885	233067.449586	37.297959
1747.771145	233455.863420	37.302976
1749.056780	233864.511695	37.307994
1751.041585	234263.697753	37.313012
1752.783790	234663.610673	37.318029
1754.278991	235075.123053	37.323047
1756.558060	235466.185613	37.328064
1757.906532	235855.040391	37.333082
1759.584762	236222.046836	37.338100
1761.433241	236604.546403	37.343117
1763.086595	236991.524311	37.348135
1764.812983	237367.923754	37.353152
1766.657406	237754.820847	37.358170
1768.101286	238132.741748	37.363188
1769.941401	238524.035605	37.368205
1771.643603	238923.735689	37.373223
1773.343169	239320.007686	37.378240
1775.074560	239714.395405	37.383258
1777.240506	240104.469892	37.388276
1778.899111	240502.808402	37.393293
1780.138894	240909.726575	37.398311
1782.368841	241316.964565	37.403328
1784.194020	241718.884797	37.408346
1785.845066	242112.146815	37.413364
1787.863272	242524.476900	37.418381
1789.165516	242944.140231	37.423399
1790.949376	243352.623758	37.428416
1792.655167	243773.923725	37.433434
1794.447262	244191.933137	37.438452
1796.250987	244612.659333	37.443469
1797.929640	245043.110638	37.448487
1799.549794	245471.362177	37.453504
1801.243682	245906.206857	37.458522
1803.029720	246336.362781	37.463540
1804.851453	246777.817643	37.468557
1806.555478	247229.352060	37.473575
1808.416611	247661.580266	37.478592
1810.202189	248110.866841	37.483610
1812.080197	248554.245172	37.488628
1814.161307	249014.686675	37.493645
1815.870413	249469.296609	37.498663
1817.912271	249904.545709	37.503680
1819.424865	250356.420042	37.508698
1821.277771	250814.309924	37.513716
1823.547096	251262.020981	37.518733
1824.934125	251717.829304	37.523751
1827.069492	252160.380939	37.528768
1828.850234	252621.916832	37.533786
1830.359412	253073.514424	37.538804
1832.462883	253535.708898	37.543821
1834.041916	253998.041057	37.548839
1836.416930	254451.300049	37.553856
1837.713505	254925.314003	37.558874
1839.974720	255382.047036	37.563892
1841.856868	255845.981160	37.568909
1843.762348	256300.131308	37.573927
1845.970764	256762.538418	37.578944
1847.605569	257220.035907	37.583962
1849.888750	257686.342944	37.588980
1852.010555	258136.799615	37.593997
1853.659471	258586.648517	37.599015
1855.415208	259042.246327	37.604032
1857.577584	259497.573731	37.609050
1859.224802	259944.476061	37.614068
1861.308390	260398.927247	37.619085
1863.122690	260860.611945	37.624103
1865.299598	261291.016005	37.629120
1866.855238	261752.057280	37.634138
1868.425223	262202.071004	37.639156
1870.711078	262656.030844	37.644173
1872.102749	263104.473229	37.649191
1874.384088	263550.050319	37.654208
1876.353169	264016.814210	37.659226
1877.937362	264466.951473	37.664244
1879.852460	264918.608794	37.669261
1882.003577	265347.287765	37.674279
1883.868992	265766.080985	37.679296
1885.580545	266203.799230	37.684314
1887.364256	266627.025433	37.689332
1888.939298	267049.625262	37.694349
1890.580698	267492.841047	37.699367
1892.767112	267922.502790	37.704384
1894.550485	268368.107550	37.709402
1896.270194	268816.084825	37.714420
1897.976480	269259.237253	37.719437
1899.281602	269716.503231	37.724455
1901.331382	270171.384809	37.729472
1903.254876	270635.965141	37.734490
1905.010577	271098.108473	37.739508
1906.786603	271550.493125	37.744525
1908.405348	272027.111915	37.749543
1910.437580	272500.359324	37.754560
1912.097579	272989.645712	37.759578
1913.936318	273477.047349	37.764596
1916.007167	273959.557898	37.769613
1917.493107	274467.998524	37.774631
1919.405354	274954.521622	37.779648
1921.441175	275452.937100	37.784666
1923.335811	275955.261428	37.789684
1925.507440	276454.947905	37.794701
1927.358428	276959.868299	37.799719
1929.277538	277472.168335	37.804736
1931.426786	277978.408848	37.809754
1933.971139	278489.968139	37.814772
1935.913854	278993.293645	37.819789
1937.589467	279493.232728	37.824807
1939.780205	279997.327583	37.829824
1941.851485	280500.780384	37.834842
1944.067715	281006.875072	37.839860
1945.885445	281511.078230	37.844877
1948.162213	282020.106667	37.849895
1950.266488	282525.936108	37.854912
1952.276380	283030.255547	37.859930
1954.382085	283531.230062	37.864948
1955.968197	284026.471948	37.869965
1958.171354	284539.772280	37.874983
1960.301979	285035.225922	37.880000
1962.378527	285531.042519	37.885018
1964.092291	286038.728844	37.890036
1966.115865	286545.168438	37.895053
1968.036820	287046.466862	37.900071
1970.387522	287551.096266	37.905088
1971.962879	288045.259838	37.910106
1973.853229	288556.718186	37.915124
1976.143807	289064.349266	37.920141
1977.738178	289586.876365	37.925159
1979.720500	290077.358460	37.930176
1981.840800	290595.857648	37.935194
1983.807464	291117.250299	37.940212
1986.031546	291624.323531	37.945229
1987.583887	292134.121779	37.950247
1989.817349	292638.852485	37.955264
1991.666130	293160.027318	37.960282
1993.706542	293682.996971	37.965300
1995.673420	294193.759323	37.970317
1997.611124	294720.170152	37.975335
1999.421653	295247.310703	37.980352
2001.597122	295756.863187	37.985370
2003.602200	296272.765765	37.990388
2005.894404	296790.294795	37.995405
2007.594961	297315.894181	38.000423
2009.528759	297838.277621	38.005440
2011.668764	298348.636352	38.010458
2013.428891	298851.258002	38.015476
2015.638522	299345.650140	38.020493
2017.632162	299842.081944	38.025511
2019.464538	300337.699753	38.030528
2021.502706	300824.722028	38.035546
2023.106920	301340.030258	38.040564
2025.024806	301849.620278	38.045581
2027.262542	302352.703810	38.050599
2029.121097	302872.355419	38.055616
2031.167194	303377.395220	38.060634
2033.237381	303898.428304	38.065652
2035.184749	304401.167579	38.070669
2037.117681	304924.934810	38.075687
2038.871516	305451.877660	38.080704
2041.048061	305979.864967	38.085722
2042.808768	306528.107642	38.090740
2045.028761	307057.782671	38.095757
2046.603581	307611.001244	38.100775
2048.991231	308149.860369	38.105792
2051.043892	308704.516482	38.110810
2053.007971	309259.513582	38.115828
2054.990344	309806.123440	38.120845
2056.993601	310362.858693	38.125863
2058.786031	310925.541806	38.130880
2060.988561	311484.851854	38.135898
2063.016339	312053.074744	38.140916
2065.464924	312618.836871	38.145933
2067.233067	313199.689579	38.150951
2069.373029	313771.360000	38.155968
2071.512270	314336.347595	38.160986
2073.590356	314915.027988	38.166004
2075.768564	315487.338921	38.171021
2078.139229	316075.052474	38.176039
2080.031064	316650.600877	38.181056
2082.308867	317229.965913	38.186074
2084.648217	317818.482619	38.191092
2086.593882	318395.912127	38.196109
2088.693508	318982.427043	38.201127
2090.715193	319566.004294	38.206144
2093.132653	320145.930912	38.211162
2095.090910	320734.739045	38.216180
2097.295209	321312.278427	38.221197
2099.504558	321899.333412	38.226215
2101.756137	322482.034284	38.231232
2104.089993	323063.395955	38.236250
2106.059764	323650.423612	38.241268
2108.164686	324226.226515	38.246285
2110.329460	324805.848042	38.251303
2112.503013	325400.797878	38.256320
2114.677288	325979.289613	38.261338
2116.684907	326574.763138	38.266356
2118.880291	327152.859288	38.271373
2121.118319	327739.219410	38.276391
2123.263290	328321.628510	38.281408
2125.422518	328897.504760	38.286426
2127.217769	329490.749772	38.291444
2129.518604	330077.025216	38.296461
2131.729054	330669.021665	38.301479
2133.876085	331253.330164	38.306496
2136.462704	331843.424320	38.311514
2138.119721	332434.554204	38.316532
2140.252310	333008.438267	38.321549
2142.704920	333596.987259	38.326567
2144.673372	334192.692367	38.331584
2147.066549	334771.363437	38.336602
2149.232149	335366.743745	38.341620
2151.385698	335941.354694	38.346637
2153.910678	336519.147269	38.351655
2155.758174	337071.051944	38.356672
2157.854296	337612.426172	38.361690
2159.933499	338176.414306	38.366708
2161.834328	338719.509816	38.371725
2164.065396	339267.900839	38.376743
2166.172470	339828.972386	38.381760
2168.177746	340394.039515	38.386778
2170.165525	340960.143795	38.391796
2172.283240	341533.987015	38.396813
2174.275837	342100.635811	38.401831
2176.054067	342687.491558	38.406848
2178.567293	343258.254223	38.411866
2180.416792	343850.769417	38.416884
2182.203998	344446.282437	38.421901
2184.750072	345033.997943	38.426919
2187.007609	345636.702416	38.431936
2188.906851	346235.930539	38.436954
2191.334528	346832.068980	38.441972
2193.539381	347437.626645	38.446989
2195.946594	348039.691448	38.452007
2197.719279	348650.177044	38.457024
2200.202425	349253.862787	38.462042
2202.089751	349872.078505	38.467060
2204.326851	350496.090021	38.472077
2206.517250	351117.892693	38.477095
2208.618849	351748.684456	38.482112
2210.786248	352372.807766	38.487130
2213.001084	353022.289849	38.492148
2215.096159	353650.035391	38.497165
2217.448438	354290.188318	38.502183
2219.810777	354939.236382	38.507200
2222.020868	355571.172138	38.512218
2224.183211	356213.788579	38.517236
2226.587115	356865.717984	38.522253
2228.766395	357511.787710	38.527271
2231.017146	358169.354598	38.532288
2233.224749	358817.784101	38.537306
2235.270960	359473.917505	38.542324
2237.495973	360121.283031	38.547341
2240.183545	360785.078162	38.552359
2242.355049	361444.076303	38.557376
2244.706358	362093.773760	38.562394
2246.738073	362754.447515	38.567412
2249.187279	363420.926831	38.572429
2251.657294	364078.486871	38.577447
2253.678809	364742.172748	38.582464
2255.939800	365397.791389	38.587482
2258.448812	366064.976073	38.592500
2261.051643	366727.288439	38.597517
2263.031393	367400.980073	38.602535
2265.199006	368065.471442	38.607552
2268.051249	368719.463424	38.612570
2270.098482	369385.295383	38.617588
2272.330141	370045.935813	38.622605
2275.055506	370705.468239	38.627623
2277.216469	371370.230673	38.632640
2279.578507	372024.878462	38.637658
2281.928619	372678.425674	38.642676
2284.168471	373336.569694	38.647693
2286.671274	373984.614803	38.652711
2289.135491	374659.993950	38.657728
2291.321760	375308.421963	38.662746
2293.780618	375969.904270	38.667764
2295.739965	376610.686597	38.672781
2298.428623	377256.865014	38.677799
2300.453836	377915.313068	38.682816
2303.171040	378563.642947	38.687834
2305.781678	379203.533793	38.692852
2307.831856	379821.900360	38.697869
2310.331103	380437.189280	38.702887
2312.164705	381052.880996	38.707904
2314.621205	381661.358773	38.712922
2316.854324	382281.221562	38.717940
2319.122937	382904.996865	38.722957
2321.008709	383507.145166	38.727975
2323.858161	384145.354514	38.732992
2325.902478	384759.116379	38.738010
2328.039386	385394.477613	38.743028
2330.196748	386024.042454	38.748045
2332.646190	386648.146639	38.753063
2334.832894	387293.754852	38.758080
2336.939214	387929.678968	38.763098
2339.243964	388582.238241	38.768116
2341.368733	389232.354634	38.773133
2344.186757	389882.266985	38.778151
2346.475371	390539.249417	38.783168
2348.533818	391202.871798	38.788186
2350.890150	391866.836220	38.793204
2353.077766	392537.226937	38.798221
2355.556519	393207.529448	38.803239
2357.640888	393883.838549	38.808256
2360.116787	394552.286662	38.813274
2362.634006	395234.120608	38.818292
2364.925575	395932.222041	38.823309
2367.462815	396599.220063	38.828327
2369.559786	397296.180867	38.833344
2372.036502	397979.326617	38.838362
2374.305013	398672.500890	38.843380
2376.386572	399368.882489	38.848397
2379.093738	400069.857465	38.853415
2381.438816	400769.151935	38.858432
2384.112817	401484.947195	38.863450
2386.310182	402197.356968	38.868468
2388.775528	402891.967649	38.873485
2391.203723	403603.391639	38.878503
2393.691097	404312.963513	38.883520
2396.185204	405022.997600	38.888538
2398.955431	405732.055847	38.893556
2401.157807	406445.091205	38.898573
2403.884972	407157.109403	38.903591
2405.906580	407874.266925	38.908608
2408.546095	408582.867600	38.913626
2411.010894	409292.187862	38.918644
2413.382890	410014.069385	38.923661
2415.927559	410728.202279	38.928679
2418.108413	411450.659179	38.933696
2420.881387	412165.045137	38.938714
2423.100962	412877.248801	38.943732
2425.469329	413600.021260	38.948749
2428.386478	414313.539877	38.953767
2430.840416	415034.688183	38.958784
2433.193986	415756.871379	38.963802
2435.545817	416463.307413	38.968820
2438.042753	417194.417251	38.973837
2440.489653	417910.319900	38.978855
2442.905987	418626.004873	38.983872
2445.398164	419349.000734	38.988890
2447.809954	420074.293448	38.993908
2450.332338	420802.788096	38.998925
2452.775323	421520.108226	39.003943
2455.367687	422243.358521	39.008960
2457.736979	422966.649828	39.013978
2460.108999	423680.045298	39.018996
2462.780415	424402.181185	39.024013
2465.512025	425117.500874	39.029031
2467.483960	425832.570461	39.034048
2470.178128	426520.614785	39.039066
2472.553682	427207.628843	39.044084
2474.925494	427890.826777	39.049101
2477.292506	428576.182944	39.054119
2479.494562	429268.786012	39.059136
2481.998246	429955.953000	39.064154
2484.336975	430648.746289	39.069172
2486.680692	431352.654909	39.074189
2489.371883	432053.549156	39.079207
2492.154816	432760.531950	39.084224
2494.073849	433467.028398	39.089242
2496.777098	434181.269761	39.094260
2499.182147	434895.841880	39.099277
2501.860080	435607.968011	39.104295
2503.994593	436329.068944	39.109312
2506.093245	437053.897971	39.114330
2509.116050	437777.842868	39.119348
2511.357229	438522.034257	39.124365
2513.729791	439252.718910	39.129383
2516.223798	439998.236539	39.134400
2518.346826	440751.178035	39.139418
2521.573804	441495.107807	39.144436
2523.395487	442248.756538	39.149453
2526.639730	443006.040570	39.154471
2529.020713	443769.866180	39.159488
2531.409778	444534.624983	39.164506
2534.194037	445298.684630	39.169524
2536.372211	446064.840826	39.174541
2538.907796	446836.879962	39.179559
2541.540814	447619.700227	39.184576
2543.953461	448397.318259	39.189594
2546.775107	449173.120703	39.194612
2549.015310	449955.869355	39.199629
2552.102845	450738.752671	39.204647
2554.391668	451532.814445	39.209664
2556.796602	452327.332696	39.214682
2559.413917	453115.211466	39.219700
2561.956038	453924.969021	39.224717
2564.372701	454719.090462	39.229735
2567.040402	455526.387854	39.234752
2569.234804	456328.220222	39.239770
2572.289565	457130.688158	39.244788
2574.996453	457947.995556	39.249805
2577.680118	458758.954227	39.254823
2580.035091	459572.007275	39.259840
2582.838488	460387.127214	39.264858
2585.462445	461199.564372	39.269876
2587.762242	462005.905517	39.274893
2590.557006	462826.740179	39.279911
2593.475938	463639.938617	39.284928
2596.235040	464460.407915	39.289946
2598.869018	465271.665213	39.294964
2601.192287	466092.036915	39.299981
2604.236257	466907.403673	39.304999
2606.691063	467734.961405	39.310016
2609.257944	468549.882784	39.315034
2611.992073	469360.093301	39.320052
2614.502994	470180.108642	39.325069
2617.310317	470989.884260	39.330087
2619.908851	471806.884575	39.335104
2622.439773	472633.106058	39.340122
2625.345922	473442.255166	39.345140
2627.657645	474260.105749	39.350157
2630.571963	475082.316907	39.355175
2633.030595	475896.889115	39.360192
2635.510052	476720.311828	39.365210
2638.518294	477528.609897	39.370228
2641.011997	478334.331072	39.375245
2643.882887	479126.874327	39.380263
2646.366764	479898.388151	39.385280
2648.868191	480673.350802	39.390298
2651.929733	481449.450361	39.395316
2654.305091	482242.393939	39.400333
2656.832199	483006.698964	39.405351
2659.527466	483789.120131	39.410368
2661.578312	484581.912885	39.415386
2664.330565	485365.467257	39.420404
2666.989615	486167.832708	39.425421
2669.521676	486957.562447	39.430439
2672.411891	487757.545873	39.435456
2674.685120	488567.740399	39.440474
2677.440674	489377.969276	39.445492
2680.000049	490199.044285	39.450509
2682.520766	491015.897907	39.455527
2685.369524	491838.765370	39.460544
2687.902122	492671.637693	39.465562
2690.668528	493495.650680	39.470580
2693.052072	494336.237915	39.475597
2695.733405	495178.954722	39.480615
2698.306720	496026.440745	39.485632
2700.687447	496883.502006	39.490650
2703.967031	497738.403933	39.495668
2706.389627	498598.952883	39.500685
2709.153377	499463.386436	39.505703
2712.070667	500321.192455	39.510720
2714.718490	501198.568994	39.515738
2717.151400	502072.807446	39.520756
2720.296755	502943.351703	39.525773
2722.991203	503821.488872	39.530791
2725.958702	504703.517748	39.535808
2728.546316	505587.124789	39.540826
2731.368342	506466.560891	39.545844
2733.902246	507348.719443	39.550861
2736.842495	508240.795784	39.555879
2739.662502	509127.448106	39.560896
2742.368864	510018.607141	39.565914
2745.390827	510909.865992	39.570932
2748.483663	511800.508725	39.575949
2750.835072	512700.145030	39.580967
2753.829640	513585.864706	39.585984
2756.438750	514483.290281	39.591002
2759.250120	515373.122315	39.596020
2762.295593	516287.859280	39.601037
2765.089349	517181.219171	39.606055
2768.249407	518073.157126	39.611072
2771.041207	518975.180878	39.616090
2774.005172	519853.797452	39.621108
2777.039300	520748.775032	39.626125
2779.629624	521639.693087	39.631143
2782.643272	522517.090470	39.636160
2785.335858	523420.077130	39.641178
2788.523308	524306.408462	39.646196
2791.479112	525191.970423	39.651213
2793.957575	526085.465290	39.656231
2797.030315	526961.536592	39.661248
2799.643743	527857.773503	39.666266
2802.433757	528732.528376	39.671284
2805.192254	529624.153478	39.676301
2808.205729	530514.675783	39.681319
2811.041301	531391.380021	39.686336
2813.798878	532287.424896	39.691354
2817.046378	533159.676519	39.696372
2819.386313	534046.319881	39.701389
2822.073803	534934.160318	39.706407
2824.966778	535815.319677	39.711424
2827.827900	536696.178814	39.716442
2830.779976	537539.229082	39.721460
2832.917546	538386.590674	39.726477
2836.016657	539242.045203	39.731495
2838.694651	540085.745009	39.736512
2841.016585	540942.030337	39.741530
2843.969530	541790.362512	39.746548
2846.333811	542662.432852	39.751565
2849.105258	543529.653864	39.756583
2851.830776	544402.964813	39.761600
2854.568636	545292.212061	39.766618
2857.143767	546169.209084	39.771636
2859.768481	547066.055707	39.776653
2862.411090	547980.641241	39.781671
2865.608665	548891.353909	39.786688
2868.056136	549803.286241	39.791706
2871.208327	550718.560703	39.796724
2873.483389	551632.309811	39.801741
2875.982532	552569.686005	39.806759
2879.087275	553507.651457	39.811776
2881.780592	554463.461458	39.816794
2884.984587	555407.812020	39.821812
2887.666270	556365.046649	39.826829
2890.364980	557334.369955	39.831847
2893.537465	558288.320656	39.836864
2896.311174	559262.314611	39.841882
2899.258469	560232.189347	39.846900
2902.499600	561212.744469	39.851917
2905.213588	562199.140006	39.856935
2907.882501	563195.664528	39.861952
2910.769819	564193.684101	39.866970
2913.726084	565182.425913	39.871988
2916.546712	566177.994046	39.877005
2919.539393	567178.779412	39.882023
2922.732478	568188.089452	39.887040
2925.670361	569197.462627	39.892058
2928.835722	570202.100421	39.897076
2931.885994	571209.689692	39.902093
2934.634580	572231.101338	39.907111
2937.896698	573236.988937	39.912128
2940.913883	574261.755450	39.917146
2944.359827	575277.436065	39.922164
2947.266043	576287.804916	39.927181
2950.164459	577300.350990	39.932199
2953.603216	578300.334632	39.937216
2956.059897	579333.456290	39.942234
2959.298860	580346.650710	39.947252
2962.450098	581357.017858	39.952269
2965.278661	582382.901426	39.957287
2968.986824	583392.457394	39.962304
2971.267640	584411.340992	39.967322
2974.177571	585423.968963	39.972340
2977.411239	586440.820510	39.977357
2980.460007	587462.128520	39.982375
2983.534735	588472.619062	39.987392
2986.687256	589498.147931	39.992410
2989.583920	590522.628765	39.997428
2992.526071	591538.194494	40.002445
2995.510572	592556.422356	40.007463
2998.523819	593562.533305	40.012480
3001.566248	594587.691340	40.017498
3004.252065	595613.420019	40.022516
3007.635000	596626.521848	40.027533
3010.306916	597651.423198	40.032551
3013.299241	598671.724419	40.037568
3016.423053	599697.823406	40.042586
3019.317099	600726.623338	40.047604
3022.450587	601748.182521	40.052621
3025.453303	602756.405836	40.057639
3028.616474	603757.405737	40.062656
3031.351928	604736.714935	40.067674
3034.473729	605708.368788	40.072692
3037.572797	606682.095314	40.077709
3040.353636	607667.950778	40.082727
3043.655704	608648.230272	40.087744
3046.718732	609626.212389	40.092762
3049.650804	610615.137227	40.097780
3052.977264	611596.806285	40.102797
3055.464577	612590.832224	40.107815
3058.082231	613582.997389	40.112832
3061.381564	614593.415433	40.117850
3064.143940	615615.481138	40.122868
3067.487562	616613.755625	40.127885
3070.355005	617640.066257	40.132903
3073.440854	618650.347292	40.137920
3076.761568	619689.688950	40.142938
3079.368659	620723.201138	40.147956
3082.616130	621758.408598	40.152973
3085.491568	622807.221100	40.157991
3088.509053	623841.367528	40.163008
3091.761630	624909.950537	40.168026
3094.935976	625948.864612	40.173044
3097.953858	627015.228003	40.178061
3100.453354	628089.112443	40.183079
3103.923641	629150.442273	40.188096
3106.845533	630237.624308	40.193114
3109.742066	631321.902377	40.198132
3113.245317	632400.426765	40.203149
3116.097551	633503.459809	40.208167
3119.487696	634596.653810	40.213184
3122.671836	635698.102562	40.218202
3125.314180	636792.387240	40.223220
3128.812603	637897.693090	40.228237
3131.758996	639017.990510	40.233255
3134.848951	640133.253103	40.238272
3138.042132	641245.783487	40.243290
3141.393720	642371.434921	40.248308
3144.660847	643489.494886	40.253325
3147.489003	644615.932164	40.258343
3150.846454	645748.340107	40.263360
3154.012194	646881.749618	40.268378
3157.301453	648024.283754	40.273396
3160.761151	649151.506427	40.278413
3163.842440	650285.492735	40.283431
3167.231948	651420.993757	40.288448
3170.572424	652545.261220	40.293466
3173.569833	653684.952992	40.298484
3177.026461	654803.165288	40.303501
3180.010252	655952.013124	40.308519
3183.423216	657101.203724	40.313536
3186.701391	658218.409126	40.318554
3189.717307	659353.057783	40.323572
3193.233040	660482.811561	40.328589
3196.053468	661632.013711	40.333607
3199.648987	662764.027183	40.338624
3202.922057	663912.335764	40.343642
3205.846813	665057.578617	40.348660
3209.276228	666181.553006	40.353677
3212.480307	667325.184596	40.358695
3215.652504	668466.843427	40.363712
3219.216967	669614.518054	40.368730
3222.159095	670752.208901	40.373748
3225.609259	671876.599866	40.378765
3228.628197	673023.651373	40.383783
3232.016063	674155.536710	40.388800
3235.108605	675288.526790	40.393818
3238.569463	676418.684061	40.398836
3241.954580	677507.962461	40.403853
3244.636513	678595.787599	40.408871
3248.364831	679679.138410	40.413888
3251.320869	680766.513409	40.418906
3254.323399	681854.447547	40.423924
3257.570838	682933.072735	40.428941
3260.560558	684038.680375	40.433959
3263.540460	685137.153593	40.438976
3266.861334	686248.943323	40.443994
3269.643087	687364.557879	40.449012
3272.800439	688480.717357	40.454029
3275.968350	689615.796289	40.459047
3279.076086	690748.161018	40.464064
3282.210869	691887.473968	40.469082
3285.498630	693042.989311	40.474100
3288.793558	694189.721559	40.479117
3291.778805	695364.679540	40.484135
3294.765480	696528.471067	40.489152
3298.097980	697697.358115	40.494170
3301.116168	698891.379054	40.499188
3304.711795	700075.326308	40.504205
3307.355349	701285.442462	40.509223
3310.479219	702485.597367	40.514240
3314.175736	703711.954503	40.519258
3317.268773	704941.507650	40.524276
3320.590216	706166.736244	40.529293
3323.660672	707402.432075	40.534311
3326.843230	708644.419537	40.539328
3330.503189	709889.119231	40.544346
3333.519837	711156.271285	40.549364
3337.182219	712406.692604	40.554381
3340.570946	713682.713155	40.559399
3343.849857	714950.838748	40.564416
3347.439697	716227.975405	40.569434
3350.356907	717503.544450	40.574452
3354.097741	718766.960777	40.579469
3357.443937	720061.558825	40.584487
3360.906575	721346.490935	40.589504
3364.222968	722627.935307	40.594522
3367.371533	723916.772521	40.599540
3371.043268	725210.759155	40.604557
3374.600485	726510.145422	40.609575
3377.729103	727804.207792	40.614592
3381.528110	729091.976557	40.619610
3384.794306	730387.137778	40.624628
3388.120962	731687.169432	40.629645
3392.081304	732990.048142	40.634663
3395.676851	734291.147098	40.639680
3399.069995	735581.356467	40.644698
3402.632817	736883.175987	40.649716
3406.008966	738181.507705	40.654733
3409.330858	739472.334162	40.659751
3412.822681	740769.188122	40.664768
3416.619960	742070.218556	40.669786
3419.424707	743367.893770	40.674804
3423.388174	744664.523004	40.679821
3426.748858	745962.368304	40.684839
3430.095079	747257.190884	40.689856
3433.992502	748553.432529	40.694874
3437.190360	749855.831322	40.699892
3440.767818	751147.799438	40.704909
3444.630170	752438.716363	40.709927
3447.834876	753720.068948	40.714944
3451.406409	755011.685359	40.719962
3454.930465	756303.091676	40.724980
3458.492736	757586.889193	40.729997
3462.017342	758874.167722	40.735015
3465.017911	760134.798254	40.740020
3468.650413	761346.339174	40.745024
3472.237272	762519.765686	40.750029
3475.389370	763618.075701	40.755034
3478.474980	764654.307280	40.760039
3481.188132	765625.775411	40.765044
3484.229973	766528.692458	40.770048
3487.311436	767382.451759	40.775053
3490.450781	768137.833008	40.780058
3492.674261	768831.147961	40.785063
3494.997209	769468.504515	40.790068
3497.547786	770032.059871	40.795072
3499.717002	770541.293299	40.800077
3501.908250	770975.064322	40.805082
3503.944660	771368.194361	40.810087
3505.254137	771714.577453	40.815092
3507.327471	771994.025190	40.820096
3508.857669	772229.073607	40.825101
3510.540110	772411.780851	40.830106
3512.228112	772554.734768	40.835111
3513.477883	772659.882424	40.840116
3514.321022	772716.236850	40.845120
3515.660611	772743.449992	40.850125
3517.090213	772724.104404	40.855130
3518.176411	772677.726159	40.860135
3518.886566	772596.932073	40.865140
3519.929077	772492.982066	40.870144
3520.300140	772353.135669	40.875149
3521.080345	772190.709057	40.880154
3521.569735	772013.648035	40.885159
3522.460781	771810.655675	40.890164
3523.167849	771578.772189	40.895168
3523.348132	771344.899209	40.900173
3523.929383	771080.261450	40.905178
3524.356694	770811.107141	40.910183
3524.848825	770538.779236	40.915188
3525.026403	770224.417070	40.920192
3525.048761	769916.620247	40.925197
3525.642017	769585.459372	40.930202
3525.957762	769248.564135	40.935207
3526.107621	768906.309595	40.940212
3526.333641	768547.616273	40.945216
3526.288611	768199.201159	40.950221
3526.382895	767824.231217	40.955226
3526.698127	767450.881761	40.960231
3526.493546	767069.219857	40.965236
3526.668036	766684.419777	40.970240
3526.680720	766304.408173	40.975245
3526.651922	765910.827084	40.980250
3526.976886	765521.751938	40.985255
3526.764015	765125.546891	40.990260
3526.781447	764711.236934	40.995264
3526.699944	764307.373814	41.000269
3526.664785	763903.185437	41.005274
3526.564941	763490.208052	41.010279
3526.270524	763100.320234	41.015284
3526.607013	762695.413837	41.020288
3526.314468	762290.934559	41.025293
3526.603683	761873.069382	41.030298
3526.630312	761463.116696	41.035303
3526.247298	761048.424226	41.040308
3526.425856	760641.460360	41.045312
3526.349426	760226.326935	41.050317
3526.172318	759809.263141	41.055322
3525.913818	759398.604101	41.060327
3525.888455	758984.479705	41.065332
3525.843779	758570.878704	41.070336
3525.337436	758166.707534	41.075341
3525.548126	757756.129096	41.080346
3525.386534	757345.935335	41.085351
3524.880771	756947.424388	41.090356
3525.210910	756538.093265	41.095360
3524.761969	756135.137537	41.100365
3524.804152	755732.326450	41.105370
3524.989826	755330.260380	41.110375
3524.748353	754930.070255	41.115380
3524.567862	754518.147929	41.120384
3524.342457	754128.232110	41.125389
3524.300565	753725.773752	41.130394
3523.496109	753334.727985	41.135399
3523.713760	752944.629707	41.140404
3523.822652	752556.356828	41.145408
3523.359197	752168.553787	41.150413
3523.249043	751792.131483	41.155418
3522.820919	751411.544865	41.160423
3522.342905	751025.563680	41.165428
3522.709356	750653.304691	41.170432
3522.648815	750285.642912	41.175437
3522.330272	749908.521028	41.180442
3522.035510	749548.273132	41.185447
3522.107138	749175.645906	41.190452
3522.089181	748814.330201	41.195456
3521.541107	748449.280384	41.200461
3521.668372	748084.448046	41.205466
3521.227613	747729.229455	41.210471
3520.982006	747383.994359	41.215476
3521.022011	747028.911720	41.220480
3520.752927	746678.756677	41.225485
3520.965374	746327.567522	41.230490
3520.949331	745975.115142	41.235495
3520.293340	745641.337647	41.240500
3520.251537	745299.832324	41.245504
3520.062943	744961.944933	41.250509
3520.114850	744624.102224	41.255514
3519.543982	744291.983464	41.260519
3519.445874	743957.745734	41.265524
3519.453667	743617.839987	41.270528
3519.196072	743297.641914	41.275533
3519.166630	742979.865509	41.280538
3518.722475	742666.397123	41.285543
3518.636035	742347.467313	41.290548
3518.676820	742037.256593	41.295552
3518.258600	741729.235823	41.300557
3518.431381	741415.616099	41.305562
3518.129559	741096.473442	41.310567
3517.827811	740801.058434	41.315572
3517.737957	740491.550490	41.320576
3517.483561	740195.907265	41.325581
3517.514498	739902.580320	41.330586
3517.484939	739612.418377	41.335591
3517.004892	739326.574359	41.340596
3516.957975	739039.857161	41.345600
3516.895251	738747.047156	41.350605
3516.754246	738467.696188	41.355610
3516.733222	738179.954264	41.360615
3516.397053	737907.641357	41.365620
3516.488915	737627.480402	41.370624
3515.952039	737351.668563	41.375629
3515.909722	737078.883100	41.380634
3515.979950	736816.807846	41.385639
3515.750385	736542.006062	41.390644
3515.901460	736277.277057	41.395648
3515.387215	736019.428932	41.400653
3515.437082	735753.264097	41.405658
3515.473053	735501.297008	41.410663
3515.065972	735238.803320	41.415668
3514.960953	734981.349307	41.420672
3514.845742	734732.154723	41.425677
3514.826522	734486.747981	41.430682
3514.756454	734237.728623	41.435687
3514.404662	733993.351622	41.440692
3514.423797	733748.609062	41.445696
3514.142083	733509.403641	41.450701
3514.197800	733259.194683	41.455706
3513.888007	733031.514612	41.460711
3513.987891	732798.958246	41.465716
3513.791352	732552.828673	41.470720
3513.651787	732327.477189	41.475725
3513.305439	732098.043898	41.480730
3513.321267	731870.723058	41.485735
3513.215555	731646.981007	41.490740
3513.515976	731420.789020	41.495744
3512.951287	731195.971232	41.500749
3512.598278	730985.126496	41.505754
3512.843872	730771.800618	41.510759
3512.661010	730552.299878	41.515764
3512.858109	730339.961091	41.520768
3512.504655	730124.240703	41.525773
3512.370286	729918.780004	41.530778
3512.543217	729714.650253	41.535783
3512.105276	729504.821141	41.540788
3512.214983	729302.771691	41.545792
3511.927438	729104.745201	41.550797
3511.633024	728900.473907	41.555802
3511.718011	728709.756799	41.560807
3511.430714	728508.743746	41.565812
3511.609158	728317.159960	41.570816
3511.392547	728126.924744	41.575821
3511.446740	727934.213082	41.580826
3511.205599	727735.105368	41.585831
3511.133419	727557.218016	41.590836
3511.187862	727372.617764	41.595840
3511.015758	727188.744278	41.600845
3510.804099	727004.724544	41.605850
3510.884599	726824.071158	41.610855
3510.345370	726657.686158	41.615860
3510.418415	726473.310288	41.620864
3510.337306	726308.626417	41.625869
3510.191813	726133.742662	41.630874
3510.151654	725968.401068	41.635879
3510.024102	725798.660460	41.640884
3510.158715	725621.242051	41.645888
3509.793366	725459.808894	41.650893
3509.692679	725295.405237	41.655898
3509.985280	725141.786139	41.660903
3509.796813	724970.304010	41.665908
3510.020653	724809.851246	41.670912
3509.840120	724649.858452	41.675917
3509.753087	724468.685257	41.680922
3510.021154	724325.462458	41.685927
3509.521652	724162.241762	41.690932
3509.684585	723997.421807	41.695936
3509.208423	723840.633995	41.700941
3509.161269	723686.548107	41.705946
3509.125867	723541.428691	41.710951
3508.832580	723392.284806	41.715956
3509.310484	723247.521738	41.720960
3508.954340	723102.843998	41.725965
3508.872007	722947.857902	41.730970
3508.901254	722806.333428	41.735975
3508.765001	722669.047280	41.740980
3508.843358	722512.539437	41.745984
3508.850953	722376.067437	41.750989
3508.837216	722222.940193	41.755994
3508.606195	722082.635979	41.760999
3508.376255	721946.245608	41.766004
3508.553311	721794.962851	41.771008
3508.508432	721672.369045	41.776013
3508.286413	721531.161636	41.781018
3508.555267	721389.028112	41.786023
3508.274686	721258.187496	41.791028
3508.230323	721125.669768	41.796032
3508.369155	720993.119739	41.801037
3508.150754	720862.758448	41.806042
3507.832466	720730.279546	41.811047
3507.633989	720603.034555	41.816052
3507.646836	720467.422773	41.821056
3507.724388	720352.623493	41.826061
3507.629511	720224.810217	41.831066
3507.663651	720099.056316	41.836071
3507.619843	719983.329812	41.841076
3507.759989	719857.604384	41.846080
3507.636284	719737.226434	41.851085
3507.836785	719612.131999	41.856090
3507.703264	719489.322245	41.861095
3507.298377	719371.167267	41.866100
3507.682079	719250.599501	41.871104
3507.522034	719127.491243	41.876109
3507.021127	719005.280400	41.881114
3507.481475	718882.859782	41.886119
3507.095845	718778.628831	41.891124
3507.260174	718660.667557	41.896128
3507.241844	718544.867296	41.901133
3507.112929	718432.059388	41.906138
3506.811603	718313.723584	41.911143
3506.673248	718211.627047	41.916148
3506.794320	718094.557655	41.921152
3506.765831	717996.110604	41.926157
3506.718769	717893.151967	41.931162
3506.626946	717794.018591	41.936167
3506.266094	717689.472373	41.941172
3506.687088	717583.903209	41.946176
3506.706868	717476.315573	41.951181
3506.219423	717373.224702	41.956186
3506.290973	717266.865892	41.961191
3506.301130	717173.859078	41.966196
3506.509313	717082.505124	41.971200
3506.241422	716981.754229	41.976205
3506.358010	716876.375129	41.981210
3506.573401	716780.304240	41.986215
3506.207252	716689.338275	41.991220
3506.047284	716586.034941	41.996224
3506.054310	716490.590348	42.001229
3506.059815	716401.693128	42.006234
3506.233581	716309.592321	42.011239
3505.904167	716217.821460	42.016244
3506.173267	716120.692395	42.021248
3505.639461	716038.875105	42.026253
3505.765223	715945.389144	42.031258
3505.650180	715856.952518	42.036263
3505.468299	715773.139828	42.041268
3505.545624	715669.786128	42.046272
3505.513798	715598.598005	42.051277
3505.540456	715520.751530	42.056282
3505.731556	715441.240001	42.061287
3505.617865	715347.489176	42.066292
3505.553061	715259.335673	42.071296
3505.678828	715179.882057	42.076301
3505.370439	715095.438471	42.081306
3505.742135	715006.763864	42.086311
3505.365157	714931.558476	42.091316
3505.022264	714836.053539	42.096320
3505.466799	714760.760878	42.101325
3505.197185	714693.970611	42.106330
3505.358270	714612.918067	42.111335
3505.138986	714541.702285	42.116340
3505.351596	714452.452643	42.121344
3505.049835	714385.069798	42.126349
3505.127747	714303.680653	42.131354
3505.506701	714216.088183	42.136359
3504.978919	714151.271357	42.141364
3505.252978	714062.950271	42.146368
3505.054267	713983.092260	42.151373
3504.993503	713907.428659	42.156378
3504.983531	713837.413002	42.161383
3505.191267	713774.159256	42.166388
3505.042894	713682.678303	42.171392
3505.027794	713613.902230	42.176397
3504.857903	713544.902982	42.181402
3504.992799	713461.412112	42.186407
3504.652082	713397.551173	42.191412
3504.784132	713322.942327	42.196416
3505.207210	713252.403840	42.201421
3504.797298	713180.413974	42.206426
3504.918877	713110.569130	42.211431
3504.684046	713042.668279	42.216436
3504.770630	712974.912433	42.221440
3504.835210	712914.703148	42.226445
3504.731332	712832.535753	42.231450
3504.714252	712760.229439	42.236455
3504.348369	712699.891041	42.241460
3504.535082	712635.838187	42.246464
3504.532407	712571.419016	42.251469
3504.677361	712505.337222	42.256474
3504.630349	712437.896880	42.261479
3504.550785	712369.170952	42.266484
3504.462364	712304.069041	42.271488
3504.507568	712248.076907	42.276493
3504.451990	712189.371231	42.281498
3504.645934	712116.975030	42.286503
3504.309151	712052.706238	42.291508
3504.427845	711988.213007	42.296512
3504.677782	711925.335579	42.301517
3504.550420	711864.058519	42.306522
3504.643202	711786.911283	42.311527
3504.193247	711733.479083	42.316532
3504.247723	711667.356041	42.321536
3504.206485	711601.943159	42.326541
3504.233488	711550.019556	42.331546
3504.097266	711491.719435	42.336551
3504.229678	711438.437599	42.341556
3504.242844	711389.195679	42.346560
3503.986346	711319.845131	42.351565
3504.193323	711278.959360	42.356570
3503.991395	711213.123225	42.361575
3503.794287	711161.532007	42.366580
3503.768503	711104.700185	42.371584
3503.964938	711044.853025	42.376589
3504.022775	710998.778383	42.381594
3504.009573	710937.575111	42.386599
3504.042753	710884.455077	42.391604
3503.778544	710833.319686	42.396608
3503.733793	710786.615476	42.401613
3503.662492	710738.674364	42.406618
3503.756594	710681.075347	42.411623
3503.844145	710635.688821	42.416628
3504.290101	710583.044947	42.421632
3503.851945	710528.064328	42.426637
3503.643585	710480.789696	42.431642
3503.757187	710421.398587	42.436647
3503.428804	710378.362790	42.441652
3503.700440	710325.051048	42.446656
3503.903427	710282.373997	42.451661
3503.666945	710227.755356	42.456666
3503.792272	710173.126390	42.461671
3503.624306	710131.254370	42.466676
3503.777534	710070.265667	42.471680
3503.973403	710030.865084	42.476685
3503.626728	709980.284254	42.481690
3503.829139	709918.889203	42.486695
3503.804147	709886.325790	42.491700
3503.950963	709827.868348	42.496704
3503.686862	709785.712596	42.501709
3503.721777	709735.514254	42.506714
3504.094301	709670.713416	42.511719
3503.616009	709631.819254	42.516724
3503.618075	709584.703569	42.521728
3503.413150	709530.919274	42.526733
3503.590051	709482.384076	42.531738
3503.806542	709438.509029	42.536743
3503.405716	709386.394500	42.541748
3503.752951	709341.951279	42.546752
3503.662939	709293.955482	42.551757
3503.341538	709261.239930	42.556762
3503.657063	709202.154615	42.561767
3503.441805	709158.150674	42.566772
3503.550012	709101.382725	42.571776
3503.387540	709057.717121	42.576781
3503.473652	709009.938961	42.581786
3503.890040	708979.235746	42.586791
3503.431454	708934.972844	42.591796
3503.702272	708886.816003	42.596800
3503.696160	708838.704522	42.601805
3503.512198	708792.012338	42.606810
3503.613770	708741.052392	42.611815
3503.384495	708704.248025	42.616820
3503.603987	708662.354612	42.621824
3503.649067	708618.304995	42.626829
3503.609540	708575.113200	42.631834
3504.143251	708509.979095	42.636839
3503.693116	708460.746965	42.641844
3503.665661	708411.345594	42.646848
3503.414585	708367.740723	42.651853
3503.303743	708320.289097	42.656858
3503.676510	708277.971310	42.661863
3503.423932	708237.295674	42.666868
3503.172818	708188.525737	42.671872
3503.274913	708153.749937	42.676877
3503.197013	708106.341354	42.681882
3503.335474	708072.949606	42.686887
3503.394996	708035.747183	42.691892
3503.320853	707987.542820	42.696896
3503.501074	707947.688315	42.701901
3503.420904	707906.982702	42.706906
3503.733033	707862.835542	42.711911
3503.323861	707832.512547	42.716916
3503.274660	707781.124819	42.721920
3503.394280	707737.753607	42.726925
3503.337512	707696.198947	42.731930
3503.496857	707653.367006	42.736935
3503.152456	707612.405582	42.741940
3503.283123	707565.356913	42.746944
3503.184996	707537.166626	42.751949
3503.137915	707487.465211	42.756954
3503.319191	707446.664673	42.761959
3503.249474	707404.812776	42.766964
3503.150214	707375.728263	42.771968
3503.078062	707333.975742	42.776973
3503.164958	707303.618795	42.781978
3503.062081	707256.507597	42.786983
3502.874144	707224.656164	42.791988
3503.155055	707184.384238	42.796993
3503.052081	707157.335716	42.801997
3502.774070	707119.936635	42.807002
3503.118234	707067.734893	42.812007
3502.894081	707045.374224	42.817012
3502.961354	707002.305899	42.822017
3502.940259	706975.590951	42.827021
3502.930831	706935.117386	42.832026
3503.012406	706904.660581	42.837031
3502.944741	706870.801495	42.842036
3503.065138	706833.434845	42.847041
3503.035252	706794.900866	42.852045
3502.774493	706761.073166	42.857050
3502.922167	706726.780719	42.862055
3503.053506	706698.301548	42.867060
3503.127253	706649.667992	42.872065
3503.114300	706616.494193	42.877069
3502.769680	706594.152200	42.882074
3502.812154	706542.294973	42.887079
3502.901829	706526.337710	42.892084
3502.969157	706492.653553	42.897089
3503.083642	706451.511645	42.902093
3502.941085	706415.875144	42.907098
3502.844107	706376.804024	42.912103
3503.023139	706345.931855	42.917108
3502.807741	706312.591579	42.922113
3502.811264	706290.042429	42.927117
3503.274751	706261.755417	42.932122
3503.120274	706214.796015	42.937127
3502.885766	706179.720025	42.942132
3503.226384	706138.440026	42.947137
3503.238173	706101.733775	42.952141
3502.920787	706076.654224	42.957146
3503.146576	706026.849738	42.962151
3502.877931	705997.788474	42.967156
3502.968159	705955.853504	42.972161
3503.137450	705914.600664	42.977165
3502.914475	705892.087795	42.982170
3503.170779	705848.287186	42.987175
3502.950263	705819.763751	42.992180
3502.956223	705774.911296	42.997185
3503.049661	705734.315798	43.002189
3502.992885	705715.301637	43.007194
3503.236902	705679.995752	43.012199
3503.203273	705648.113055	43.017204
3502.835848	705595.026243	43.022209
3502.671614	705571.012736	43.027213
3502.483213	705531.704494	43.032218
3502.777515	705506.075450	43.037223
3502.937565	705474.905266	43.042228
3503.001588	705444.595207	43.047233
3502.912452	705411.926040	43.052237
3502.645013	705372.878457	43.057242
3502.597860	705350.384872	43.062247
3502.626428	705318.292019	43.067252
3502.676952	705298.315486	43.072257
3502.745794	705251.562400	43.077261
3502.748907	705233.878470	43.082266
3503.060897	705192.548994	43.087271
3502.659739	705170.659675	43.092276
3502.671503	705139.214676	43.097281
3502.913852	705097.945897	43.102285
3502.590543	705071.721905	43.107290
3502.891887	705045.543926	43.112295
3502.725442	705013.780118	43.117300
3502.916956	704980.317963	43.122305
3502.832080	704947.397965	43.127309
3502.469437	704919.391715	43.132314
3502.808189	704887.792571	43.137319
3502.694788	704866.749209	43.142324
3502.578328	704839.894330	43.147329
3502.862322	704805.720811	43.152333
3502.724382	704783.985839	43.157338
3502.897831	704744.266659	43.162343
3502.596098	704723.552034	43.167348
3502.681410	704682.207796	43.172353
3502.773082	704655.715457	43.177357
3502.228536	704643.435893	43.182362
3502.778027	704597.146504	43.187367
3502.372998	704587.327688	43.192372
3502.605590	704546.803034	43.197377
3502.934172	704523.102819	43.202381
3502.699718	704487.622524	43.207386
3503.069757	704458.897926	43.212391
3502.820237	704435.143698	43.217396
3502.727960	704394.175088	43.222401
3502.996950	704364.125533	43.227405
3502.594533	704333.043916	43.232410
3503.070455	704293.421861	43.237415
3502.914920	704277.451172	43.242420
3502.696235	704233.422581	43.247425
3502.971133	704208.786463	43.252429
3502.725413	704178.622364	43.257434
3502.829326	704134.887867	43.262439
3502.709771	704119.904537	43.267444
3502.598699	704072.479216	43.272449
3503.055596	704042.745340	43.277453
3502.895344	704030.004141	43.282458
3502.474840	703991.720729	43.287463
3502.492716	703968.318596	43.292468
3502.355354	703934.608512	43.297473
3502.517422	703909.195253	43.302477
3502.431645	703881.885220	43.307482
3502.810131	703854.399241	43.312487
3502.803829	703838.899957	43.317492
3502.699527	703796.887207	43.322497
3503.029699	703772.737553	43.327501
3502.899458	703742.602586	43.332506
3502.985597	703702.942700	43.337511
3502.479840	703676.297402	43.342516
3502.726465	703652.707679	43.347521
3502.880714	703616.613262	43.352525
3502.693960	703588.524033	43.357530
3502.673327	703544.459304	43.362535
3502.256809	703527.238491	43.367540
3502.260486	703497.925209	43.372545
3502.262645	703467.320324	43.377549
3502.432209	703453.729003	43.382554
3502.890765	703430.948366	43.387559
3502.776453	703402.796914	43.392564
3502.670898	703365.949334	43.397569
3503.060047	703341.242245	43.402573
3502.583717	703301.027319	43.407578
3502.621838	703280.253233	43.412583
3502.873458	703254.972354	43.417588
3502.398407	703221.961035	43.422593
3502.611620	703206.225712	43.427597
3502.812967	703177.127196	43.432602
3502.564388	703138.563260	43.437607
3502.678109	703118.819710	43.442612
3502.885237	703084.552707	43.447617
3502.987115	703045.533129	43.452621
3502.615151	703027.409645	43.457626
3502.623266	702990.392683	43.462631
3502.556357	702963.225705	43.467636
3502.571317	702939.672221	43.472641
3502.625845	702906.771180	43.477645
3502.409732	702901.291684	43.482650
3502.542418	702858.688792	43.487655
3502.161844	702841.858182	43.492660
3502.276778	702822.560937	43.497665
3502.989202	702788.954805	43.502669
3502.499255	702763.496571	43.507674
3502.690263	702735.044209	43.512679
3502.819730	702714.949338	43.517684
3502.470405	702677.542758	43.522689
3502.821439	702652.144371	43.527693
3502.778709	702623.928910	43.532698
3502.859868	702584.960367	43.537703
3502.677314	702559.649634	43.542708
3502.557280	702526.129972	43.547713
3502.981923	702492.371365	43.552717
3502.792525	702469.595607	43.557722
3502.444574	702427.169177	43.562727
3502.723361	702410.676279	43.567732
3502.817454	702386.064789	43.572737
3502.972685	702354.685426	43.577741
3502.534652	702321.416131	43.582746
3502.950914	702288.602214	43.587751
3502.604420	702255.069133	43.592756
3503.071948	702225.873886	43.597761
3502.743621	702196.809680	43.602765
3502.472398	702176.233000	43.607770
3503.030664	702136.885691	43.612775
3502.407014	702105.385320	43.617780
3502.480863	702078.142691	43.622785
3502.763044	702049.325229	43.627789
3502.568761	702029.381505	43.632794
3502.815216	701993.314847	43.637799
3502.584105	701972.035395	43.642804
3502.722049	701941.054921	43.647809
3502.633330	701911.999972	43.652813
3502.836141	701883.294424	43.657818
3502.897103	701855.009690	43.662823
3502.909827	701819.825594	43.667828
3502.798058	701794.351892	43.672833
3502.904141	701767.898060	43.677837
3502.788767	701727.318207	43.682842
3502.402912	701697.267954	43.687847
3502.431644	701668.192839	43.692852
3502.560489	701644.468002	43.697857
3502.706432	701605.285626	43.702861
3502.688466	701599.623573	43.707866
3502.896697	701573.152319	43.712871
3502.779464	701538.982375	43.717876
3502.488614	701508.965511	43.722881
3502.724017	701482.787669	43.727885
3502.414918	701462.464011	43.732890
3503.006162	701419.182184	43.737895
3502.759019	701404.563052	43.742900
3502.432757	701374.004916	43.747905
3502.539108	701340.940334	43.752909
3502.436338	701333.503063	43.757914
3502.602079	701299.583723	43.762919
3502.398698	701282.323327	43.767924
3502.421931	701246.886709	43.772929
3502.609366	701223.846812	43.777933
3502.387758	701200.576081	43.782938
3502.589104	701166.252789	43.787943
3502.535373	701142.954242	43.792948
3502.571362	701117.901480	43.797953
3502.651078	701094.829297	43.802957
3502.635004	701068.343776	43.807962
3502.491472	701032.884072	43.812967
3502.841113	701021.346549	43.817972
3502.669072	700991.208930	43.822977
3502.531288	700957.487366	43.827981
3502.603266	700927.855988	43.832986
3502.573799	700901.421865	43.837991
3502.367211	700878.247193	43.842996
3502.805783	700847.213298	43.848001
3502.688677	700819.053944	43.853005
3502.535321	700805.660800	43.858010
3503.077848	700765.017759	43.863015
3502.786067	700741.310081	43.868020
3502.705353	700709.267899	43.873025
3502.828938	700672.619649	43.878029
3502.662843	700641.634962	43.883034
3502.835194	700616.309797	43.888039
3502.548039	700587.879523	43.893044
3502.625034	700564.359093	43.898049
3502.853132	700531.619282	43.903053
3502.368079	700507.893117	43.908058
3502.335631	700467.691336	43.913063
3502.774082	700454.796536	43.918068
3502.515234	700420.695247	43.923073
3502.495315	700398.731048	43.928077
3502.560123	700365.272016	43.933082
3502.659912	700336.926266	43.938087
3502.480488	700315.037840	43.943092
3502.649306	700291.799752	43.948097
3502.468671	700262.605351	43.953101
3502.311408	700233.257897	43.958106
3502.689323	700197.162162	43.963111
3502.701095	700179.416816	43.968116
3502.650158	700157.109210	43.973121
3502.682261	700126.189440	43.978125
3502.603491	700106.222280	43.983130
3502.511405	700073.782025	43.988135
3502.525865	700044.455344	43.993140
3502.740687	700009.628269	43.998145
3502.724669	699993.179391	44.003149
3502.299606	699975.853532	44.008154
3502.559775	699947.082469	44.013159
3502.534421	699927.801940	44.018164
3502.389498	699901.632333	44.023169
3502.825991	699871.788202	44.028173
3502.689155	699845.120060	44.033178
3502.815470	699814.780108	44.038183
3502.441465	699804.652524	44.043188
3502.445252	699766.032067	44.048193
3502.883344	699746.823885	44.053197
3502.361066	699711.918269	44.058202
3502.821439	699678.540544	44.063207
3502.774335	699654.342255	44.068212
3502.480972	699619.647073	44.073217
3502.967696	699590.091936	44.078221
3502.897253	699565.996660	44.083226
3502.987898	699524.080288	44.088231
3502.782080	699489.618691	44.093236
3502.917936	699469.962651	44.098241
3502.867466	699426.379074	44.103245
3502.624992	699403.057284	44.108250
3502.617029	699367.220541	44.113255
3502.610003	699346.941589	44.118260
3502.732943	699329.225908	44.123265
3502.963195	699291.261932	44.128269
3502.709555	699259.392054	44.133274
3502.709448	699227.977352	44.138279
3502.361141	699199.154979	44.143284
3502.573984	699163.082189	44.148289
3502.523365	699145.842103	44.153293
3502.060759	699133.491503	44.158298
3502.334224	699104.814902	44.163303
3502.358093	699076.576999	44.168308
3502.316296	699059.683245	44.173313
3502.439964	699022.580705	44.178317
3502.206365	699011.931981	44.183322
3502.298039	698977.270223	44.188327
3502.735400	698972.227358	44.193332
3502.437479	698932.360523	44.198337
3502.460449	698915.604945	44.203341
3501.975166	698898.435997	44.208346
3502.434837	698873.953212	44.213351
3502.422355	698850.840599	44.218356
3502.197555	698825.227737	44.223361
3502.668701	698810.784154	44.228365
3502.363693	698769.575594	44.233370
3502.629651	698750.642150	44.238375
3502.410593	698728.408318	44.243380
3502.092515	698710.266960	44.248385
3502.875280	698672.258976	44.253389
3502.421226	698652.499470	44.258394
3502.252965	698618.923044	44.263399
3502.624091	698602.904869	44.268404
3502.555397	698579.751093	44.273409
3502.568623	698551.314412	44.278413
3502.484363	698523.341101	44.283418
3502.566989	698498.472003	44.288423
3502.622195	698461.278950	44.293428
3502.691981	698444.763316	44.298433
3503.040649	698417.066310	44.303437
3502.351948	698385.215230	44.308442
3502.804735	698357.451167	44.313447
3502.473256	698338.068449	44.318452
3502.878005	698310.610427	44.323457
3502.936527	698275.901652	44.328461
3502.768712	698263.849232	44.333466
3502.938458	698225.492921	44.338471
3502.733101	698197.190537	44.343476
3502.402934	698156.231806	44.348481
3502.881897	698133.533455	44.353485
3502.692930	698114.027333	44.358490
3502.489799	698074.190692	44.363495
3502.448116	698047.004264	44.368500
3502.297873	698017.797374	44.373505
3502.760698	698003.552698	44.378509
3502.601010	697974.943789	44.383514
3502.506933	697943.887976	44.388519
3502.553272	697928.618094	44.393524
3502.502797	697910.182414	44.398529
3502.786738	697873.794331	44.403533
3502.441148	697858.489479	44.408538
3502.561637	697821.630967	44.413543
3502.872664	697792.198175	44.418548
3502.573141	697772.063213	44.423553
3502.690125	697729.089915	44.428557
3502.615508	697712.298409	44.433562
3502.598858	697670.689166	44.438567
3502.478931	697650.723196	44.443572
3502.633080	697627.182179	44.448577
3502.685655	697590.383606	44.453581
3502.605872	697571.952046	44.458586
3502.607864	697548.783907	44.463591
3502.531262	697530.103153	44.468596
3502.213285	697504.302924	44.473601
3502.500201	697468.956731	44.478605
3502.340719	697465.502869	44.483610
3502.261863	697427.382913	44.488615
3502.486406	697404.923481	44.493620
3502.409829	697382.613046	44.498625
3502.427214	697353.426045	44.503629
3502.449225	697346.611150	44.508634
3502.266488	697304.281778	44.513639
3502.217081	697286.838973	44.518644
3502.481626	697255.025585	44.523649
3502.519079	697239.507381	44.528653
3502.465028	697204.614059	44.533658
3502.186916	697185.667468	44.538663
3502.592012	697158.006927	44.543668
3502.705549	697136.907509	44.548673
3502.747231	697104.533676	44.553677
3502.414418	697078.684924	44.558682
3502.448474	697053.620871	44.563687
3502.763201	697027.068635	44.568692
3502.546513	697004.183695	44.573697
3502.758278	696967.455729	44.578701
3502.463862	696942.196886	44.583706
3502.751169	696915.400233	44.588711
3502.653311	696891.053537	44.593716
3502.328639	696870.174850	44.598721
3502.476380	696837.732840	44.603725
3502.265963	696820.365363	44.608730
3502.281579	696789.287403	44.613735
3502.308282	696770.140528	44.618740
3502.667384	696750.789675	44.623745
3502.615637	696720.567830	44.628749
3502.284101	696711.722412	44.633754
3502.108953	696690.868383	44.638759
3502.427612	696669.783770	44.643764
3502.224497	696646.249285	44.648769
3502.647978	696616.197382	44.653773
3502.427657	696590.328660	44.658778
3502.319062	696568.866713	44.663783
3502.651557	696544.448146	44.668788
3502.260709	696523.281208	44.673793
3502.279708	696492.301089	44.678797
3502.270619	696475.148369	44.683802
3502.476846	696457.910414	44.688807
3502.469264	696428.028348	44.693812
3502.576484	696401.806763	44.698817
3502.650673	696374.049128	44.703821
3502.477710	696357.718753	44.708826
3502.473543	696327.885508	44.713831
3502.580080	696308.575307	44.718836
3502.149539	696286.171252	44.723841
3502.556731	696256.966115	44.728845
3502.303137	696237.764825	44.733850
3502.522788	696217.491032	44.738855
3502.443889	696179.763482	44.743860
3502.000751	696167.306037	44.748865
3502.654661	696138.755996	44.753869
3502.597097	696116.041428	44.758874
3502.608852	696089.834649	44.763879
3502.607600	696059.502771	44.768884
3502.239524	696032.562812	44.773889
3502.404063	696005.684182	44.778893
3502.139784	695985.042071	44.783898
3502.120764	695960.083111	44.788903
3502.193242	695951.568158	44.793908
3502.396746	695921.152340	44.798913
3502.611172	695897.696232	44.803917
3502.192608	695888.814600	44.808922
3502.226907	695860.117133	44.813927
3502.355971	695845.526178	44.818932
3502.577588	695814.112486	44.823937
3502.426072	695792.059007	44.828941
3502.538722	695759.569096	44.833946
3502.484057	695741.278751	44.838951
3502.331411	695706.246572	44.843956
3502.171367	695702.991015	44.848961
3502.193231	695671.261642	44.853965
3502.218653	695658.626814	44.858970
3502.282158	695636.935334	44.863975
3502.456227	695602.147270	44.868980
3502.341596	695592.767709	44.873985
3502.578947	695549.266691	44.878989
3502.480779	695540.083273	44.883994
3502.572383	695511.076864	44.888999
3502.362044	695492.612744	44.894004
3502.707993	695464.459377	44.899009
3502.572659	695450.209709	44.904013
3502.470627	695415.864235	44.909018
3502.535805	695393.923242	44.914023
3502.477315	695358.575799	44.919028
3502.334988	695342.188769	44.924033
3502.293901	695306.589606	44.929037
3502.032293	695295.940991	44.934042
3502.140371	695271.356979	44.939047
3502.343080	695248.348647	44.944052
3502.244286	695229.666680	44.949057
3502.338606	695210.256636	44.954061
3502.158872	695187.211706	44.959066
3502.393037	695168.126635	44.964071
3502.469874	695141.906325	44.969076
3502.304004	695122.340043	44.974081
3502.696669	695087.066366	44.979085
3502.433517	695086.264357	44.984090
3502.495044	695053.531628	44.989095
3502.669696	695024.062366	44.994100
3502.249724	695007.521543	44.999105
3502.546942	694987.580271	45.004109
3502.441836	694964.423001	45.009114
3502.658543	694942.406190	45.014119
3502.431580	694901.465060	45.019124
3502.356175	694877.705893	45.024129
3502.326096	694854.486241	45.029133
3502.366438	694836.874614	45.034138
3502.202921	694817.008879	45.039143
3502.648160	694785.654158	45.044148
3502.177295	694768.524489	45.049153
3502.514362	694738.480462	45.054157
3502.664589	694722.839794	45.059162
3502.510512	694688.997402	45.064167
3502.434927	694662.900257	45.069172
3502.350680	694630.339185	45.074177
3501.973661	694624.135006	45.079181
3501.905699	694597.588815	45.084186
3502.227184	694569.933974	45.089191
3502.344896	694563.399564	45.094196
3502.180575	694534.631065	45.099201
3502.407224	694511.915281	45.104205
3502.133091	694507.186073	45.109210
3502.241116	694479.416923	45.114215
3502.112572	694458.798615	45.119220
3501.948221	694440.523657	45.124225
3501.858364	694411.891691	45.129229
3502.141652	694406.523502	45.134234
3502.341308	694390.426497	45.139239
3502.197402	694363.046636	45.144244
3502.015904	694353.776249	45.149249
3501.945991	694330.512054	45.154253
3502.064341	694317.462125	45.159258
3501.906823	694302.219569	45.164263
3502.233810	694284.509879	45.169268
3502.035640	694265.891989	45.174273
3502.258447	694256.505144	45.179277
3501.978041	694245.609686	45.184282
3502.000261	694212.034834	45.189287
3501.929526	694205.033860	45.194292
3502.072550	694193.123595	45.199297
3502.180905	694170.078282	45.204301
3502.218527	694144.508047	45.209306
3502.307557	694129.522983	45.214311
3502.483618	694102.487480	45.219316
3502.292203	694085.061759	45.224321
3502.455394	694061.857922	45.229325
3502.366930	694038.297602	45.234330
3502.416928	694014.217040	45.239335
3502.241133	694002.508263	45.244340
3502.084893	693977.168437	45.249345
3502.174153	693954.324658	45.254349
3502.127884	693944.534192	45.259354
3501.945878	693913.180279	45.264359
3502.011575	693894.368919	45.269364
3501.910933	693894.485022	45.274369
3502.378572	693861.183608	45.279373
3502.032443	693858.455404	45.284378
3502.231782	693839.572169	45.289383
3502.123760	693811.040733	45.294388
3502.082861	693793.440424	45.299393
3502.190150	693774.621957	45.304397
3502.138065	693749.811435	45.309402
3501.954432	693725.818327	45.314407
3502.404788	693706.296592	45.319412
3501.883441	693692.853774	45.324417
3502.296429	693670.204612	45.329421
3502.304217	693655.232136	45.334426
3502.068768	693623.886009	45.339431
3502.486413	693613.770043	45.344436
3502.183150	693585.270054	45.349441
3502.258482	693564.267902	45.354445
3502.299882	693550.931095	45.359450
3502.383682	693519.382777	45.364455
3502.683070	693504.312258	45.369460
3502.073315	693482.477756	45.374465
3502.441777	693451.877079	45.379469
3502.231820	693435.447927	45.384474
3502.331481	693413.496359	45.389479
3502.246708	693386.302701	45.394484
3502.213274	693384.816059	45.399489
3502.380889	693366.334968	45.404493
3502.530569	693337.809290	45.409498
3502.150261	693322.552023	45.414503
3502.349543	693287.104113	45.419508
3502.061630	693263.425383	45.424513
3502.201167	693247.982847	45.429517
3502.145543	693226.901997	45.434522
3502.109984	693217.208447	45.439527
3502.139008	693207.603726	45.444532
3502.134384	693177.809698	45.449537
3501.873109	693159.150144	45.454541
3502.023962	693158.229992	45.459546
3501.896584	693117.562670	45.464551
3502.191965	693098.114884	45.469556
3501.859774	693102.347952	45.474561
3501.907975	693071.848484	45.479565
3501.881000	693066.779326	45.484570
3501.723518	693043.973869	45.489575
3502.172549	693029.723501	45.494580
3501.986577	693015.478263	45.499585
3502.260887	692995.635790	45.504589
3502.242121	692970.618636	45.509594
3502.096829	692953.829743	45.514599
3502.521443	692939.682740	45.519604
3501.783511	692913.888568	45.524609
3502.063593	692892.154697	45.529613
3502.057221	692886.883071	45.534618
3501.933149	692872.876118	45.539623
3502.162138	692842.694276	45.544628
3502.075999	692837.485507	45.549633
3502.340505	692811.277141	45.554637
3502.302140	692790.490872	45.559642
3502.051178	692787.547679	45.564647
3502.408599	692756.697720	45.569652
3501.913603	692734.345032	45.574657
3502.231306	692721.558376	45.579661
3502.188434	692695.848013	45.584666
3502.239392	692676.190865	45.589671
3502.261986	692659.025545	45.594676
3502.121410	692638.355251	45.599681
3502.359400	692618.368693	45.604685
3502.076901	692598.567344	45.609690
3502.332206	692582.706626	45.614695
3502.175557	692552.438115	45.619700
3502.192337	692541.143379	45.624705
3502.538428	692519.298235	45.629709
3502.433770	692492.851297	45.634714
3502.072357	692474.107316	45.639719
3502.230611	692451.198569	45.644724
3502.176121	692431.011060	45.649729
3502.217852	692414.886766	45.654733
3502.584990	692400.002203	45.659738
3502.128354	692377.642296	45.664743
3502.381539	692348.996909	45.669748
3502.109401	692337.003337	45.674753
3502.525569	692311.166478	45.679757
3502.438476	692283.571869	45.684762
3502.225974	692260.226265	45.689767
3502.825881	692229.583261	45.694772
3502.599514	692220.716009	45.699777
3502.588538	692182.263826	45.704781
3502.334383	692172.406173	45.709786
3502.284727	692143.262815	45.714791
3502.846049	692113.620709	45.719796
3502.656587	692089.972380	45.724801
3502.330309	692062.068269	45.729805
3502.379674	692042.210998	45.734810
3502.512258	692017.713453	45.739815
3502.538346	691986.766192	45.744820
3502.267430	691945.171968	45.749825
3502.245054	691862.942013	45.754829
3501.920177	691736.932316	45.759834
3502.160216	691556.152579	45.764839
3501.906395	691310.077396	45.769844
3501.713566	691008.809344	45.774849
3501.511015	690649.468712	45.779853
3501.193459	690238.136282	45.784858
3500.938877	689762.733664	45.789863
3501.102072	689244.590327	45.794868
3500.257047	688666.117658	45.799873
3499.920236	688017.249549	45.804877
3499.848997	687327.725703	45.809882
3498.999208	686567.145525	45.814887
3498.698118	685766.884157	45.819892
3498.014246	684901.842878	45.824897
3497.581939	683972.645710	45.829901
3496.688947	682990.943598	45.834906
3495.888273	681960.463555	45.839911
3495.508966	680851.100512	45.844916
3494.889962	679708.615746	45.849921
3493.827139	678480.917662	45.854925
3493.176728	677224.137999	45.859930
3492.155869	675901.566159	45.864935
3491.200948	674521.227203	45.869940
3489.959803	673083.303850	45.874945
3489.346022	671586.672571	45.879949
3488.360701	670047.478163	45.884954
3486.983156	668438.971247	45.889959
3486.204975	666775.969356	45.894964
3484.808594	665071.717861	45.899969
3483.651535	663296.063798	45.904973
3482.231595	661485.936483	45.909978
3480.686220	659615.236919	45.914983
3479.628147	657695.614649	45.919988
3477.914012	655736.370454	45.924993
3476.650176	653706.580591	45.929997
3475.156605	651645.335912	45.935002
3473.492098	649514.481042	45.940007
3472.290642	647352.156554	45.945012
3470.203226	645145.818981	45.950017
3468.460094	642885.288769	45.955021
3466.737194	640596.794930	45.960026
3464.978031	638239.959334	45.965031
3463.369041	635845.281950	45.970036
3460.951433	633417.803454	45.975041
3459.183033	630947.302271	45.980045
3457.195889	628445.763069	45.985050
3455.075721	625891.667141	45.990055
3453.133399	623291.092299	45.995060
3450.706932	620677.893408	46.000065
3448.657694	618002.302913	46.005069
3446.490329	615300.559590	46.010074
3444.329497	612558.036245	46.015079
3442.277638	609779.406568	46.020084
3439.692613	606971.478597	46.025089
3437.552553	604122.482649	46.030093
3434.979789	601245.690786	46.035098
3432.724889	598336.697123	46.040103
3430.109096	595391.628530	46.045108
3427.757790	592419.856216	46.050113
3425.194635	589391.749121	46.055117
3422.404017	586343.713755	46.060122
3419.615326	583269.119080	46.065127
3417.182481	580169.654612	46.070132
3414.024971	577056.603877	46.075137
3411.981763	573896.204495	46.080141
3409.074720	570728.260024	46.085146
3406.158260	567523.235836	46.090151
3403.403430	564288.133757	46.095156
3400.333527	561039.386644	46.100161
3397.555066	557749.137307	46.105165
3394.416100	554441.052999	46.110170
3391.721797	551120.541426	46.115175
3388.528314	547768.602523	46.120180
3385.572984	544411.523842	46.125185
3382.635997	541007.940160	46.130189
3379.660424	537599.760003	46.135194
3376.379528	534167.203790	46.140199
3373.319581	530717.395585	46.145204
3369.731322	527243.288881	46.150209
3366.789636	523766.700033	46.155213
3363.244144	520253.398723	46.160218
3360.072928	516738.976952	46.165223
3356.649450	513202.376588	46.170228
3353.230428	509653.407450	46.175233
3349.745805	506091.932854	46.180237
3346.414041	502527.325151	46.185242
3343.028399	498948.097227	46.190247
3339.933064	495350.451529	46.195252
3336.196725	491741.068804	46.200257
3333.320528	488110.799589	46.205261
3329.491273	484478.113671	46.210266
3325.947824	480835.780488	46.215271
3322.739943	477176.810534	46.220276
3318.855973	473512.161127	46.225281
3315.466477	469827.717848	46.230285
3311.794029	466140.076926	46.235290
3308.412645	462442.566813	46.240295
3304.678422	458724.910458	46.245300
3300.588246	455026.094757	46.250305
3297.309453	451309.697035	46.255309
3293.576888	447586.325733	46.260314
3289.999554	443867.555882	46.265319
3286.309835	440117.479264	46.270324
3282.678100	436383.455253	46.275329
3278.648299	432641.424643	46.280333
3275.202648	428896.310344	46.285338
3271.050133	425142.245463	46.290343
3267.192599	421386.943416	46.295348
3263.389808	417632.893962	46.300353
3259.642515	413870.639317	46.305357
3255.732476	410121.202737	46.310362
3251.613427	406364.468343	46.315367
3247.845238	402615.570717	46.320372
3244.124455	398863.549744	46.325377
3240.270262	395098.816824	46.330381
3236.383660	391355.646084	46.335386
3232.548849	387601.410341	46.340391
3228.676623	383845.055616	46.345396
3224.489452	380091.190665	46.350401
3220.963501	376347.194307	46.355405
3216.654069	372596.360844	46.360410
3213.009336	368854.305420	46.365415
3209.135788	365096.623025	46.370420
3204.917853	361377.162113	46.375425
3201.016785	357629.903190	46.380429
3197.194205	353904.371361	46.385434
3192.829119	350171.658250	46.390439
3189.225942	346440.083540	46.395444
3184.944054	342728.498995	46.400449
3181.220019	339007.274657	46.405453
3177.129614	335307.698616	46.410458
3172.773055	331590.296049	46.415463
3169.098569	327887.703352	46.420468
3164.981406	324189.608525	46.425473
3161.197075	320488.845557	46.430477
3157.230032	316805.953937	46.435482
3152.848187	313129.199617	46.440487
3149.158608	309453.753968	46.445492
3145.101003	305794.953660	46.450497
3141.174055	302133.786705	46.455501
3137.049804	298481.573685	46.460506
3132.689344	294838.384880	46.465511
3128.895659	291202.114381	46.470516
3124.641825	287585.651285	46.475521
3120.826202	283960.618599	46.480525
3116.865243	280354.831437	46.485530
3112.661416	276754.693595	46.490535
3108.842742	273153.746325	46.495540
3104.460431	269561.631524	46.500545
3100.811088	265981.457864	46.505549
3096.861824	262422.142793	46.510554
3092.842727	258848.080524	46.515559
3088.803709	255284.996832	46.520564
3084.649605	251740.940899	46.525569
3080.558654	248194.399017	46.530573
3076.446803	244668.622548	46.535578
3072.170756	241141.157520	46.540583
3068.233181	237633.171270	46.545588
3064.006889	234140.753133	46.550593
3060.293150	230644.859338	46.555597
3056.244823	227168.991903	46.560602
3051.914843	223700.316747	46.565607
3048.252272	220229.087132	46.570612
3044.178130	216789.688139	46.575617
3040.099723	213344.706644	46.580621
3035.942178	209920.925106	46.585626
3031.510547	206396.531971	46.590631
3027.873045	202984.553278	46.595636
3023.489298	199582.389230	46.600641
3019.655784	196197.127501	46.605645
3015.697050	192830.210114	46.610650
3011.209393	189461.614593	46.615655
3006.732379	186104.064000	46.620660
3002.816269	182767.298847	46.625665
2999.162688	179438.114830	46.630669
2995.272738	176120.635256	46.635674
2990.709364	172822.572559	46.640679
2986.846333	169530.576115	46.645684
2982.625845	166255.513465	46.650689
2978.486835	162980.018038	46.655693
2974.847517	159730.714051	46.660698
2970.670221	156484.895403	46.665703
2966.775899	153249.886443	46.670708
2962.565256	150041.228779	46.675713
2958.400533	146820.669058	46.680717
2953.980909	143631.596310	46.685722
2949.997504	140444.682946	46.690727
2946.324290	137270.304166	46.695732
2942.067993	134121.792102	46.700737
2938.272575	130973.087039	46.705741
2934.074880	127840.528623	46.710746
2929.461355	124721.961886	46.715751
2926.120772	121612.436153	46.720756
2921.544951	118527.042516	46.725761
2917.438729	115443.105398	46.730765
2913.599530	112381.278632	46.735770
2909.105768	109335.923216	46.740775
2905.257375	106296.553610	46.745780
2901.166875	103282.874008	46.750785
2896.998667	100256.477903	46.755789
2892.691880	97268.681813	46.760794
2888.409300	94294.213639	46.765799
2884.594916	91334.480456	46.770804
2880.143804	88392.660329	46.775809
2876.031111	85464.709912	46.780813
2871.946759	82551.588569	46.785818
2867.990450	79657.301454	46.790823
2863.665453	76765.771753	46.795828
2859.341043	73915.386193	46.800833
2855.007159	71073.163632	46.805837
2850.479728	68242.319182	46.810842
2845.855391	65444.165611	46.815847
2841.723415	62660.613395	46.820852
2836.957215	59918.454232	46.825857
2832.590235	57187.501521	46.830861
2827.530911	54500.533920	46.835866
2822.540577	51837.968412	46.840871
2816.631676	49231.313933	46.845876
2807.942672	46725.393261	46.850881
2799.269232	44319.111632	46.855885
2790.521073	42003.340019	46.860890
2781.365691	39777.333903	46.865895
2773.057146	37654.315570	46.870900
2764.832341	35646.619756	46.875905
2757.752989	33719.476766	46.880909
2750.270978	31913.781550	46.885914
2743.420542	30190.126732	46.890919
2736.812831	28551.210671	46.895924
2730.198179	27011.049752	46.900929
2723.919132	25542.169991	46.905933
2718.065494	24164.011455	46.910938
2712.386036	22862.636487	46.915943
2707.356154	21614.571071	46.920948
2701.955829	20425.213897	46.925953
2696.952317	19306.442145	46.930957
2692.205386	18227.775906	46.935962
2687.242136	17209.323667	46.940967
2682.722310	16230.053636	46.945972
2678.222732	15295.327423	46.950977
2674.441259	14402.995235	46.955981
2669.880980	13530.702692	46.960986
2665.392764	12707.064939	46.965991
2661.474823	11909.626039	46.970996
2657.369714	11139.308235	46.976001
2653.435852	10389.824465	46.981005
2649.112682	9670.599525	46.986010
2644.938067	8986.563079	46.991015
2640.675265	8317.622500	46.996020
2635.829641	7698.264153	47.001025
2631.406290	7101.167036	47.006029
2626.967656	6527.410126	47.011034
2621.770687	5985.919017	47.016039
2617.823430	5473.489569	47.021044
2613.323891	4997.520446	47.026049
2608.716352	4526.254652	47.031053
2604.764991	4099.716366	47.036058
2600.379895	3684.728490	47.041063
2596.070822	3287.653621	47.046068
2591.720084	2931.019315	47.051073
2588.239154	2569.012151	47.056077
2584.146204	2235.274235	47.061082
2580.401206	1922.597517	47.066087
2576.945089	1606.664026	47.071092
2573.194594	1319.252404	47.076097
2569.363589	1038.141478	47.081101
2565.639251	783.309948	47.086106
2561.714950	525.009973	47.091111
2557.937155	280.110954	47.096116
2551.177870	134.794210	47.101121
2538.295597	175.921583	47.106125
2531.252340	168.231407	47.111130
2527.033243	184.909832	47.116135
2524.709658	170.832068	47.121140
2523.564652	178.974119	47.126145
2521.893441	182.223329	47.131149
2520.155489	174.808416	47.136154
2517.125355	179.038325	47.141159
2514.383317	172.173956	47.146164
2510.809622	179.835941	47.151169
2507.219921	174.180479	47.156173
2504.325607	171.498623	47.161178
2500.763700	178.358255	47.166183
2497.925548	174.902833	47.171188
2494.315422	179.339786	47.176193
2491.128612	184.800533	47.181197
2488.066981	173.058574	47.186202
2484.309009	181.782689	47.191207
2481.381600	177.206314	47.196212
2478.138351	182.648361	47.201217
2474.743520	175.977805	47.206221
2471.716914	166.974298	47.211226
2468.031720	172.188549	47.216231
2464.968570	166.961662	47.221236
2461.123913	166.144088	47.226241
2457.479752	167.410686	47.231245
2454.704090	160.889362	47.236250
2451.292464	163.864832	47.241255
2447.933232	159.790754	47.246260
2444.154851	169.547190	47.251265
2440.910586	160.733562	47.256269
2437.937835	149.023955	47.261274
2434.097892	154.370924	47.266279
2430.654252	158.394633	47.271284
2427.039372	150.281582	47.276289
2423.203133	160.716954	47.281293
2419.993812	158.941239	47.286298
2416.886825	160.586891	47.291303
2413.706180	146.215166	47.296308
2409.884130	154.834450	47.301313
2406.324791	155.074333	47.306317
2403.498430	156.635780	47.311322
2399.976410	154.844996	47.316327
2396.938740	147.990046	47.321332
2392.790371	157.174123	47.326337
2389.121956	159.867991	47.331341
2386.205208	150.933644	47.336346
2383.105312	152.232800	47.341351
2379.118459	158.739358	47.346356
2375.280457	152.840433	47.351361
2372.153868	153.163420	47.356365
2368.884751	158.224982	47.361370
2364.993830	162.555632	47.366375
2362.031258	151.168233	47.371380
2358.158381	157.436352	47.376385
2354.623931	159.980055	47.381389
2351.556357	147.174155	47.386394
2347.828109	160.068168	47.391399
2344.885082	161.487680	47.396404
2341.161322	161.630035	47.401409
2337.430618	153.708059	47.406413
2333.658646	156.948328	47.411418
2330.142171	155.374938	47.416423
2327.218439	157.522419	47.421428
2323.590780	158.433744	47.426433
2320.468269	154.609782	47.431437
2316.947948	148.961378	47.436442
2313.210175	160.007911	47.441447
2309.861397	154.029260	47.446452
2305.899550	156.725058	47.451457
2302.578266	157.358284	47.456461
2299.136027	159.994353	47.461466
2295.635805	163.504346	47.466471
2292.566482	150.928678	47.471476
2288.976324	156.726284	47.476481
2285.660447	160.059619	47.481485
2282.028999	148.429472	47.486490
2278.344666	156.185443	47.491495
2275.211337	151.447445	47.496500
2271.617808	153.389798	47.501505
2268.175110	158.635189	47.506509
2264.569033	154.873342	47.511514
2260.832241	158.164690	47.516519
2257.608786	152.317339	47.521524
2253.854934	152.704695	47.526529
2250.605480	146.669830	47.531533
2247.108644	152.450673	47.536538
2243.342156	152.967012	47.541543
2240.239027	147.128424	47.546548
2236.323948	144.981734	47.551553
2233.061157	154.195937	47.556557
2230.043838	145.119646	47.561562
2226.413148	149.956626	47.566567
2222.734283	144.332304	47.571572
2219.190114	145.330562	47.576577
2215.660397	150.457938	47.581581
2212.123765	141.007606	47.586586
2208.525765	143.026322	47.591591
2205.734506	138.261695	47.596596
2201.894072	142.325611	47.601601
2198.100681	154.371844	47.606605
2194.827300	148.007072	47.611610
2191.142102	154.984739	47.616615
2187.887513	146.211892	47.621620
2184.615292	144.144202	47.626625
2180.745632	148.544886	47.631629
2177.522031	139.922241	47.636634
2173.577245	140.221794	47.641639
2170.088301	134.248640	47.646644
2167.159871	142.574498	47.651649
2163.451235	137.655501	47.656653
2159.946539	138.005931	47.661658
2156.074563	145.882950	47.666663
2153.023655	137.272855	47.671668
2149.267357	141.722727	47.676673
2145.966517	143.859566	47.681677
2142.469955	139.661771	47.686682
2138.783359	139.044900	47.691687
2135.421049	136.928579	47.696692
2132.066287	144.488334	47.701697
2128.360179	137.204033	47.706701
2125.221525	138.734124	47.711706
2121.509142	147.955731	47.716711
2117.775064	143.471564	47.721716
2114.466997	146.367598	47.726721
2111.129729	144.041727	47.731725
2107.441908	142.059100	47.736730
2103.661903	146.151396	47.741735
2100.518318	138.405399	47.746740
2096.810914	133.189851	47.751745
2093.001371	140.289743	47.756749
2089.880119	136.606636	47.761754
2086.501095	147.131501	47.766759
2083.106709	147.235251	47.771764
2079.521845	146.708978	47.776769
2075.898694	140.120258	47.781773
2073.149712	136.190187	47.786778
2069.003224	149.270654	47.791783
2065.709283	138.586859	47.796788
2062.023133	136.813961	47.801793
2058.364693	138.428354	47.806797
2055.010360	144.816879	47.811802
2050.983268	144.374907	47.816807
2047.759215	140.013777	47.821812
2044.541079	135.985571	47.826817
2040.928342	142.414213	47.831821
2037.767723	135.907603	47.836826
2033.724131	141.112663	47.841831
2030.567173	146.800023	47.846836
2027.444436	143.082865	47.851841
2023.489416	151.111440	47.856845
2020.274331	140.957536	47.861850
2016.445212	147.091586	47.866855
2013.558108	140.459504	47.871860
2009.962547	140.949175	47.876865
2005.825249	138.264925	47.881869
2002.305043	137.457283	47.886874
1998.639310	150.978982	47.891879
1995.694574	147.905374	47.896884
1992.253671	140.279799	47.901889
1988.435920	141.135344	47.906893
1985.210438	135.199929	47.911898
1981.656335	134.277919	47.916903
1978.036325	134.257979	47.921908
1974.910794	133.816556	47.926913
1971.053077	139.646130	47.931917
1967.380408	134.321349	47.936922
1963.590516	130.498934	47.941927
1960.699851	128.435282	47.946932
1957.265703	134.991761	47.951937
1953.439971	139.583487	47.956941
1950.046138	143.153301	47.961946
1946.558089	137.639382	47.966951
1943.549129	133.603932	47.971956
1939.396588	132.081231	47.976961
1935.748283	135.238217	47.981965
1932.655110	129.741776	47.986970
1929.178086	130.574637	47.991975
1925.724277	137.500843	47.996980
1922.213896	129.411417	48.001985
1918.747155	135.495744	48.006989
1915.086533	128.740878	48.011994
1911.167233	138.325762	48.016999
1908.043494	126.932775	48.022004
1904.837579	132.061535	48.027009
1901.273406	128.092761	48.032013
1898.279268	125.373711	48.037018
1893.888193	133.022493	48.042023
1890.406015	120.537457	48.047028
1886.778829	124.403974	48.052033
1883.431310	132.048326	48.057037
1880.142946	133.399450	48.062042
1876.666352	126.545151	48.067047
1873.480426	122.855120	48.072052
1869.441102	119.443209	48.077057
1866.069547	125.864094	48.082061
1862.813852	118.032016	48.087066
1858.882485	126.033507	48.092071
1855.733426	131.173034	48.097076
1852.173651	121.110945	48.102081
1848.431248	134.921466	48.107085
1845.051573	129.058200	48.112090
1841.414861	141.104036	48.117095
1837.896583	126.029804	48.122100
1834.414577	129.995516	48.127105
1831.192294	134.362339	48.132109
1827.604107	124.259970	48.137114
1824.038574	127.635433	48.142119
1820.561734	129.151923	48.147124
1817.154093	122.899611	48.152129
1813.737846	137.823929	48.157133
1810.276837	132.940885	48.162138
1806.607665	137.251108	48.167143
1803.284323	134.414423	48.172148
1799.415309	133.932540	48.177153
1796.025872	138.414816	48.182157
1793.028405	133.632419	48.187162
1789.058050	133.974204	48.192167
1785.673515	131.076797	48.197172
1782.132942	128.024605	48.202177
1778.346548	134.997956	48.207181
1774.955376	122.181849	48.212186
1771.366378	133.746033	48.217191
1767.911642	120.240277	48.222196
1764.483495	120.026000	48.227201
1761.106294	127.624417	48.232205
1757.528223	120.845590	48.237210
1754.046836	121.590694	48.242215
1750.916017	116.096462	48.247220
1747.377268	120.034310	48.252225
1743.441928	129.012975	48.257229
1740.529540	115.515132	48.262234
1736.166434	132.255138	48.267239
1732.829321	123.551546	48.272244
1729.298792	126.073135	48.277249
1725.645469	135.913966	48.282253
1722.821293	123.514149	48.287258
1718.823661	123.365970	48.292263
1715.512122	129.495239	48.297268
1712.130964	119.309434	48.302273
1708.281602	126.256333	48.307277
1705.164375	115.226330	48.312282
1701.782054	120.202017	48.317287
1697.936960	123.090158	48.322292
1694.837671	121.871217	48.327297
1691.095763	120.175910	48.332301
1687.702279	120.641317	48.337306
1683.943184	126.659054	48.342311
1680.230218	126.557412	48.347316
1676.950850	122.002832	48.352321
1673.345409	118.022118	48.357325
1670.051052	117.655364	48.362330
1666.433991	133.725927	48.367335
1663.324976	117.630900	48.372340
1659.621421	115.579600	48.377345
1655.650640	116.403072	48.382349
1652.629632	115.907692	48.387354
1649.124263	115.822688	48.392359
1645.729815	120.384625	48.397364
1641.993420	120.412590	48.402369
1638.185513	124.405251	48.407373
1634.977452	105.464831	48.412378
1631.311254	119.974488	48.417383
1628.283020	112.010486	48.422388
1624.492215	116.890719	48.427393
1620.630402	124.140286	48.432397
1617.602722	113.107199	48.437402
1613.723360	121.043642	48.442407
1610.654807	112.251576	48.447412
1607.170270	117.503715	48.452417
1603.553850	116.975916	48.457421
1599.792543	108.781216	48.462426
1596.478501	115.972450	48.467431
1593.063794	122.526345	48.472436
1589.814848	120.513253	48.477441
1586.425764	118.583705	48.482445
1582.646681	116.275385	48.487450
1578.848208	128.977816	48.492455
1575.232220	126.474418	48.497460
1571.937913	121.248477	48.502465
1568.246864	127.131126	48.507469
1565.176289	119.627448	48.512474
1561.326159	116.080159	48.517479
1557.821605	121.902001	48.522484
1554.385664	116.796175	48.527489
1550.856636	120.209020	48.532493
1547.283301	115.421517	48.537498
1544.024751	115.783229	48.542503
1540.349826	110.023267	48.547508
1537.204788	108.874748	48.552513
1533.420487	108.916440	48.557517
1530.070426	112.881277	48.562522
1526.495693	121.551467	48.567527
1522.919389	114.898054	48.572532
1519.304151	123.868977	48.577537
1515.376271	118.650693	48.582541
1512.566073	111.306497	48.587546
1508.899808	116.278916	48.592551
1505.424949	111.518589	48.597556
1502.151131	118.024789	48.602561
1497.987409	120.979558	48.607565
1495.054067	114.344827	48.612570
1491.337533	120.041706	48.617575
1488.134882	119.655387	48.622580
1484.804413	119.456747	48.627585
1480.592514	124.107520	48.632589
1477.523288	114.560057	48.637594
1473.482283	110.763580	48.642599
1470.262078	110.546925	48.647604
1467.010218	118.784115	48.652609
1463.235720	115.301176	48.657613
1460.147919	106.836239	48.662618
1456.620430	122.541643	48.667623
1452.689157	113.615215	48.672628
1449.019677	109.872208	48.677633
1446.011795	112.989818	48.682637
1442.143576	112.342143	48.687642
1438.634157	119.646875	48.692647
1435.115381	108.771468	48.697652
1431.891705	110.542799	48.702657
1428.073445	112.825627	48.707661
1424.897077	111.567711	48.712666
1421.514590	121.881987	48.717671
1417.861555	121.244943	48.722676
1414.698632	116.961798	48.727681
1410.589332	116.699138	48.732685
1407.336225	113.475017	48.737690
1403.696473	113.762881	48.742695
1399.776597	114.686692	48.747700
1396.742069	119.278310	48.752705
1393.353031	111.973430	48.757709
1390.564108	105.352993	48.762714
1386.735166	115.725885	48.767719
1382.787970	121.885245	48.772724
1379.159965	110.440664	48.777729
1375.868171	113.632872	48.782733
1372.361240	113.082817	48.787738
1368.880918	114.589555	48.792743
1365.124921	113.284220	48.797748
1361.913356	109.472701	48.802753
1358.038086	125.104225	48.807757
1354.772066	104.803523	48.812762
1351.245953	115.423575	48.817767
1347.679041	112.450482	48.822772
1344.356594	112.724820	48.827777
1340.649153	119.209459	48.832781
1337.580851	109.024161	48.837786
1333.757592	118.852490	48.842791
1330.076339	110.139616	48.847796
1326.996906	106.708850	48.852801
1323.337212	116.011279	48.857805
1319.979041	109.034069	48.862810
1316.087744	108.783609	48.867815
1312.700139	103.304918	48.872820
1309.085342	106.517017	48.877825
1305.495467	112.080612	48.882829
1302.268632	106.623305	48.887834
1298.776135	107.146014	48.892839
1295.425276	109.506595	48.897844
1292.024533	95.472969	48.902849
1288.288369	107.920783	48.907853
1284.905674	103.124878	48.912858
1281.185413	114.959316	48.917863
1277.390530	107.030351	48.922868
1274.209097	108.310344	48.927873
1270.568945	108.544704	48.932877
1267.488759	114.404536	48.937882
1263.779149	112.982096	48.942887
1260.081716	111.491735	48.947892
1256.582829	113.689542	48.952897
1252.957172	116.080387	48.957901
1250.037308	108.884351	48.962906
1246.288697	106.597328	48.967911
1242.862491	109.551559	48.972916
1239.434760	114.914940	48.977921
1235.609031	113.711226	48.982925
1232.115648	111.272301	48.987930
1228.347246	117.577066	48.992935
1225.033767	113.005580	48.997940
1221.945915	109.785458	49.002945
1217.972751	113.235067	49.007949
1214.604257	111.382123	49.012954
1210.936693	110.744688	49.017959
1207.654747	111.012626	49.022964
1204.321635	102.341377	49.027969
1200.613396	110.320286	49.032973
1197.247813	104.151512	49.037978
1193.489113	110.142114	49.042983
1190.341921	109.179493	49.047988
1186.661563	105.920008	49.052993
1183.202669	116.619833	49.057997
1179.903355	106.736890	49.063002
1176.023164	112.210245	49.068007
1172.774070	109.761171	49.073012
1168.906344	108.244576	49.078017
1165.217696	114.757219	49.083021
1162.104025	108.958663	49.088026
1158.806205	112.123403	49.093031
1155.178432	107.216960	49.098036
1151.495039	106.760978	49.103041
1148.265219	112.536496	49.108045
1144.879767	107.897448	49.113050
1141.026883	104.512605	49.118055
1137.726076	106.038182	49.123060
1133.875836	107.807540	49.128065
1130.374373	114.600657	49.133069
1126.887904	114.298224	49.138074
1123.678995	111.902532	49.143079
1120.557156	105.108414	49.148084
1116.843582	101.538152	49.153089
1113.319504	106.279558	49.158093
1109.340895	110.553448	49.163098
1105.748644	105.614139	49.168103
1102.497566	106.908923	49.173108
1099.276426	90.428206	49.178113
1095.685229	109.122551	49.183117
1092.238118	104.963600	49.188122
1088.614283	107.083524	49.193127
1085.090741	106.797121	49.198132
1081.413434	109.770690	49.203137
1077.385235	110.921271	49.208141
1074.417205	95.622404	49.213146
1071.198818	109.425901	49.218151
1067.320198	102.524697	49.223156
1064.527015	95.364884	49.228161
1060.681422	110.743244	49.233165
1056.930531	101.793493	49.238170
1053.261770	106.525321	49.243175
1049.698483	107.645621	49.248180
1046.725040	107.119689	49.253185
1042.733680	117.701240	49.258189
1039.761724	104.330035	49.263194
1036.139268	111.368188	49.268199
1032.294475	112.721535	49.273204
1028.902345	106.765673	49.278209
1025.758679	106.643041	49.283213
1022.454301	92.796982	49.288218
1018.325626	97.223831	49.293223
1014.778692	103.960608	49.298228
1011.222766	101.207585	49.303233
1007.770352	109.903878	49.308237
1004.703242	96.724073	49.313242
1000.888842	102.957678	49.318247
997.341976	96.863843	49.323252
994.240182	103.809607	49.328257
990.651894	105.481498	49.333261
987.140363	107.140304	49.338266
983.441602	110.106843	49.343271
979.642716	103.089131	49.348276
976.320635	107.574243	49.353281
972.924909	109.819140	49.358285
969.651572	104.267364	49.363290
965.984060	110.729495	49.368295
962.067601	106.655768	49.373300
959.035350	97.453272	49.378305
955.379595	105.232461	49.383309
951.950916	100.823117	49.388314
948.514198	100.019847	49.393319
944.787753	98.766617	49.398324
941.859851	94.482258	49.403329
937.940588	103.823541	49.408333
934.414046	102.023592	49.413338
930.899406	107.197119	49.418343
927.441269	107.181622	49.423348
924.144413	94.851723	49.428353
919.988952	105.272441	49.433357
917.119657	97.060295	49.438362
913.300211	100.553805	49.443367
909.481209	98.519464	49.448372
906.490423	92.911933	49.453377
902.893049	103.984911	49.458381
899.699722	103.807433	49.463386
895.916660	105.101746	49.468391
892.457311	104.428755	49.473396
889.035145	96.343988	49.478401
885.268788	110.412865	49.483405
881.773214	101.671864	49.488410
878.304045	99.278159	49.493415
874.706861	102.262122	49.498420
871.261135	102.456358	49.503425
867.489325	99.029935	49.508429
864.275236	96.597802	49.513434
861.046533	95.845839	49.518439
857.618986	107.919275	49.523444
854.089323	103.332535	49.528449
849.890321	108.368109	49.533453
846.683675	97.875748	49.538458
843.307691	108.512348	49.543463
839.808560	105.784014	49.548468
836.582796	104.469963	49.553473
832.761310	105.191503	49.558477
829.326030	115.528304	49.563482
826.018375	105.496670	49.568487
822.170484	111.095999	49.573492
819.013183	107.035558	49.578497
815.269203	104.559289	49.583501
811.825244	107.213072	49.588506
808.359077	102.203040	49.593511
804.364534	104.095608	49.598516
801.448020	100.547697	49.603521
797.819173	96.746826	49.608525
794.515632	108.510891	49.613530
791.019220	98.482296	49.618535
787.077175	106.498409	49.623540
783.701602	94.973169	49.628545
780.242302	101.908741	49.633549
776.741772	105.132934	49.638554
773.247993	97.111024	49.643559
769.819063	103.601916	49.648564
766.441950	97.803041	49.653569
762.744523	98.550098	49.658573
759.458339	93.841663	49.663578
755.659346	92.718406	49.668583
751.937311	95.470724	49.673588
748.659117	87.788905	49.678593
744.947408	92.130638	49.683597
742.114292	96.586528	49.688602
738.522092	91.114133	49.693607
734.765595	95.608129	49.698612
731.174144	97.413160	49.703617
727.262781	93.230671	49.708621
724.164730	102.751609	49.713626
720.726673	100.941537	49.718631
716.977305	96.016126	49.723636
714.068031	83.385302	49.728641
710.086550	91.527777	49.733645
706.990178	92.710422	49.738650
703.494990	95.354210	49.743655
699.529929	96.308595	49.748660
696.660456	92.155050	49.753665
692.432168	100.433886	49.758669
689.307718	97.470232	49.763674
685.805245	89.872929	49.768679
681.789985	99.482487	49.773684
678.623647	91.461350	49.778689
674.862187	96.443634	49.783693
671.709588	85.600308	49.788698
668.280746	91.445571	49.793703
664.560914	97.689055	49.798708
661.263483	88.121792	49.803713
657.527575	98.903106	49.808717
654.024355	88.915826	49.813722
650.735695	89.777487	49.818727
647.492316	91.568805	49.823732
643.653023	100.349875	49.828737
639.906580	91.260271	49.833741
636.360232	88.302328	49.838746
633.180881	94.034311	49.843751
629.380249	99.880339	49.848756
626.478472	84.846178	49.853761
622.539037	97.251122	49.858765
619.383305	91.311945	49.863770
615.501811	87.844894	49.868775
611.969082	93.869400	49.873780
608.650085	89.788715	49.878785
605.212952	91.154699	49.883789
601.699426	82.830346	49.888794
598.160682	96.468068	49.893799
594.098658	88.603096	49.898804
591.702943	75.014193	49.903809
587.595478	86.049036	49.908813
584.399889	84.067138	49.913818
580.624673	83.637483	49.918823
576.720019	91.084576	49.923828
573.478278	80.623129	49.928833
570.011379	93.516669	49.933837
566.447205	84.463285	49.938842
563.006043	87.589803	49.943847
559.836243	88.414893	49.948852
556.254698	83.718399	49.953857
552.720493	94.443324	49.958861
548.852070	85.452140	49.963866
545.495992	78.959105	49.968871
541.688154	85.965341	49.973876
538.618361	81.704752	49.978881
534.999574	89.545618	49.983885
531.402088	87.983098	49.988890
528.044346	86.927725	49.993895
524.452515	89.998889	49.998900
521.312783	83.675104	50.003905
517.436462	88.356442	50.008909
513.838582	73.681284	50.013914
510.410689	81.199507	50.018919
506.857098	84.090899	50.023924
504.111248	81.411651	50.028929
500.098005	88.867105	50.033933
496.946186	91.270906	50.038938
493.035786	86.884436	50.043943
489.292531	87.510446	50.048948
486.039951	79.450069	50.053953
482.179943	83.522918	50.058957
478.896553	82.452714	50.063962
475.453356	91.935996	50.068967
471.778659	90.839187	50.073972
468.383564	75.717096	50.078977
464.590508	85.482255	50.083981
461.514672	80.116860	50.088986
458.265579	97.204504	50.093991
454.624277	92.039053	50.098996
451.102211	91.514731	50.104001
447.212190	92.903296	50.109005
443.958326	84.466846	50.114010
440.793230	88.355856	50.119015
436.785374	86.829955	50.124020
432.873227	81.547931	50.129025
429.834509	90.636925	50.134029
426.584721	89.977379	50.139034
422.987826	81.808277	50.144039
419.260023	88.870828	50.149044
416.115183	82.135345	50.154049
412.573135	83.608234	50.159053
408.963389	82.541382	50.164058
405.622777	85.242303	50.169063
401.696398	87.701942	50.174068
398.338252	76.985224	50.179073
394.595534	83.432011	50.184077
391.461883	79.323197	50.189082
387.798661	81.965242	50.194087
384.293559	83.907418	50.199092
381.002738	77.224543	50.204097
377.002159	77.347213	50.209101
373.881323	85.691670	50.214106
370.563704	83.085438	50.219111
366.950062	89.897267	50.224116
363.856332	80.822448	50.229121
360.073966	90.518038	50.234125
356.544257	89.291165	50.239130
352.568913	85.662688	50.244135
348.953509	85.150544	50.249140
345.627153	86.265144	50.254145
342.256253	88.689529	50.259149
338.988269	86.085763	50.264154
335.726334	80.334496	50.269159
331.764422	84.140376	50.274164
328.599965	81.859292	50.279169
324.509917	83.323897	50.284173
321.244832	82.282358	50.289178
318.052150	71.676857	50.294183
314.379324	84.037900	50.299188
311.034953	84.169821	50.304193
307.325873	83.021226	50.309197
303.899055	92.881193	50.314202
300.305009	80.607763	50.319207
296.723339	83.466081	50.324212
293.306504	81.242193	50.329217
289.778451	79.105390	50.334221
285.912764	76.997051	50.339226
282.695337	82.477455	50.344231
279.419782	88.904430	50.349236
275.723234	77.325246	50.354241
272.100236	79.089693	50.359245
268.853452	83.196190	50.364250
265.497370	77.454450	50.369255
261.602761	79.673533	50.374260
258.365733	76.819816	50.379265
254.816889	82.954604	50.384269
251.429508	76.250328	50.389274
247.852905	81.620309	50.394279
244.236447	90.849258	50.399284
240.727593	73.476673	50.404289
236.719448	78.017072	50.409293
233.666200	74.849381	50.414298
230.333954	77.076826	50.419303
226.938149	88.353110	50.424308
223.506005	80.717350	50.429313
219.714037	90.124162	50.434317
216.138474	78.764176	50.439322
212.677652	80.996542	50.444327
209.075253	90.684558	50.449332
205.923075	82.511100	50.454337
202.010678	85.902191	50.459341
198.910996	84.766469	50.464346
195.063561	74.429308	50.469351
191.603101	80.597464	50.474356
187.997687	73.774236	50.479361
184.531997	80.725101	50.484365
181.123618	81.240091	50.489370
177.733312	78.786551	50.494375
174.253494	78.191725	50.499380
171.171668	83.230816	50.504385
167.352402	80.581507	50.509389
163.678157	76.470808	50.514394
160.262914	79.702271	50.519399
156.501057	82.553041	50.524404
153.302376	76.910052	50.529409
149.667335	81.341791	50.534413
146.340863	82.261991	50.539418
142.608323	77.457072	50.544423
138.953836	88.033281	50.549428
135.499111	77.002452	50.554433
132.133677	82.369529	50.559437
128.489451	82.216759	50.564442
125.366289	83.664927	50.569447
121.676412	86.226357	50.574452
118.272132	76.678645	50.579457
114.661602	84.916090	50.584461
111.037217	81.327617	50.589466
107.558403	74.401805	50.594471
103.516489	88.323263	50.599476
100.817519	79.385369	50.604481
97.241980	78.169067	50.609485
93.677503	72.137366	50.614490
90.267020	74.277231	50.619495
86.374386	76.202904	50.624500
83.088345	69.369716	50.629505
79.361076	73.548801	50.634509
75.921853	81.948533	50.639514
73.127042	76.630642	50.644519
69.482286	78.236652	50.649524
65.638635	79.551576	50.654529
61.892415	77.541472	50.659533
58.456869	73.872841	50.664538
55.240160	75.007001	50.669543
51.280412	85.222379	50.674548
47.877764	76.462219	50.679553
44.282486	82.551381	50.684557
41.172828	75.632383	50.689562
37.668643	68.887255	50.694567
33.980422	70.705324	50.699572
30.623208	70.018091	50.704577
27.138067	69.904186	50.709581
23.902755	71.680812	50.714586
20.312356	82.333123	50.719591
16.573834	75.930315	50.724596
13.016250	73.847579	50.729601
9.275494	78.423231	50.734605
5.734536	70.556851	50.739610
2.720145	72.152264	50.744615