Tue Jun 21 11:04:56 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.126219	81.164816	0.000000
-0.076257	81.832874	0.005005
-0.265484	84.128683	0.010010
-0.281607	71.481541	0.015014
-0.045899	57.547138	0.020019
-0.677282	63.181044	0.025024
-1.022845	50.220050	0.030029
-0.984393	41.485502	0.035034
-1.681395	36.620298	0.040038
-1.388780	30.728285	0.045043
-2.023689	18.385129	0.050048
-1.973057	9.088354	0.055053
-2.547865	-1.324364	0.060058
-2.962186	-4.367031	0.065062
-3.019023	-14.441050	0.070067
-3.063723	-11.908116	0.075072
-3.535912	-20.260297	0.080077
-4.000750	-15.782344	0.085082
-4.505154	-20.374345	0.090086
-5.185671	-23.673071	0.095091
-5.496121	-12.809351	0.100096
-5.418661	-25.687397	0.105101
-5.819330	-20.644651	0.110106
-5.754825	-20.923833	0.115110
-5.496033	-19.677445	0.120115
-6.046510	-12.613278	0.125120
-6.005488	-4.473716	0.130125
-6.781270	-8.813978	0.135130
-7.172678	-11.727830	0.140134
-6.939417	-19.732504	0.145139
-7.257917	-11.046789	0.150144
-7.559842	-22.680387	0.155149
-8.116447	-16.228516	0.160154
-8.749501	-18.562055	0.165158
-8.498712	-18.297452	0.170163
-9.042714	-11.762419	0.175168
-8.948245	-20.057869	0.180173
-8.816334	-9.990228	0.185178
-8.902257	-13.379128	0.190182
-9.692558	-12.635669	0.195187
-10.506984	-11.761528	0.200192
-10.368535	-11.922123	0.205197
-10.439505	-15.596079	0.210202
-10.960043	-11.691822	0.215206
-10.454856	-13.758996	0.220211
-10.936749	-14.405706	0.225216
-11.793046	-7.917623	0.230221
-11.960707	-10.477807	0.235226
-12.068985	-8.749921	0.240230
-12.143972	-15.283942	0.245235
-12.404420	-14.658810	0.250240
-12.392684	-25.416883	0.255245
-13.317970	-20.153865	0.260250
-13.869506	-12.405963	0.265254
-13.465428	-13.067172	0.270259
-13.710219	-14.112291	0.275264
-13.660758	-17.485326	0.280269
-13.459709	-7.691783	0.285274
-14.405420	-7.899779	0.290278
-14.898370	-15.102020	0.295283
-15.027141	-6.284921	0.300288
-15.299455	-12.276360	0.305293
-15.309757	-12.651292	0.310298
-15.458437	-3.385319	0.315302
-16.231234	-9.625597	0.320307
-16.814395	-8.904598	0.325312
-16.541601	-8.449070	0.330317
-16.851729	-7.309355	0.335322
-17.014262	-5.809480	0.340326
-16.784649	-17.573330	0.345331
-17.240817	-9.880685	0.350336
-17.977855	-14.052522	0.355341
-18.439182	-7.804285	0.360346
-18.428582	-6.936524	0.365350
-18.450220	-16.015300	0.370355
-18.735355	-15.034631	0.375360
-18.299646	-19.226621	0.380365
-18.974188	-10.083730	0.385370
-19.718725	-15.344389	0.390374
-19.762721	-5.883620	0.395379
-19.868638	-13.157648	0.400384
-20.311468	-10.324157	0.405389
-20.295667	-9.987885	0.410394
-21.264932	-1.288528	0.415398
-21.274609	-14.749281	0.420403
-21.710213	-9.759945	0.425408
-21.650450	-19.797026	0.430413
-22.073794	-17.725112	0.435418
-21.883000	-10.940575	0.440422
-22.077238	-15.074228	0.445427
-21.857572	-13.375587	0.450432
-22.248784	-13.337967	0.455437
-22.981520	-17.284568	0.460442
-23.162159	-12.306867	0.465446
-23.512845	-13.917961	0.470451
-23.556984	-5.838102	0.475456
-24.286632	-16.371979	0.480461
-24.771665	-11.243231	0.485466
-25.247213	-13.134975	0.490470
-24.801354	-19.629544	0.495475
-25.431731	-14.741746	0.500480
-25.075808	-15.012947	0.505485
-25.085027	-13.192340	0.510490
-25.520959	-8.648526	0.515494
-25.473202	-15.194584	0.520499
-26.455936	-16.715219	0.525504
-26.872851	-15.739170	0.530509
-26.717317	-9.855537	0.535514
-26.854481	-6.202623	0.540518
-26.612653	-19.240499	0.545523
-27.401595	-17.555198	0.550528
-27.708854	-19.772781	0.555533
-28.020719	-17.246913	0.560538
-28.192367	-13.422531	0.565542
-28.476514	-15.830619	0.570547
-28.939557	-8.537025	0.575552
-29.281427	-11.027906	0.580557
-29.413019	-12.617857	0.585562
-29.656655	-10.267468	0.590566
-29.504756	-12.617919	0.595571
-29.468055	1.100161	0.600576
-29.899541	-12.258380	0.605581
-30.534420	-5.951012	0.610586
-30.806535	-8.692217	0.615590
-30.739023	-7.790468	0.620595
-31.311712	-14.874125	0.625600
-32.046292	-17.564594	0.630605
-32.201037	-16.341289	0.635610
-32.746572	-8.967336	0.640614
-31.658058	-19.219572	0.645619
-32.500486	-13.138119	0.650624
-32.490458	-14.281082	0.655629
-32.522167	-13.528661	0.660634
-33.255073	-6.606551	0.665638
-33.653623	-14.580994	0.670643
-34.421408	-7.521290	0.675648
-34.287313	-16.450228	0.680653
-34.083978	-17.827270	0.685658
-34.497627	-8.350676	0.690662
-34.151717	-19.678338	0.695667
-35.198427	-20.675312	0.700672
-35.580125	-16.475354	0.705677
-35.690223	-18.037093	0.710682
-36.033970	-9.036793	0.715686
-35.536222	-18.477053	0.720691
-35.744334	-12.747308	0.725696
-36.614307	-12.504307	0.730701
-37.118256	-14.444231	0.735706
-37.009735	-13.700627	0.740710
-37.272993	-15.787364	0.745715
-37.544123	-14.251943	0.750720
-37.662671	-18.663934	0.755725
-38.132349	-12.780565	0.760730
-38.388803	-11.117138	0.765734
-38.838040	-14.157173	0.770739
-39.260623	-16.047424	0.775744
-39.446660	-18.199636	0.780749
-39.721771	-14.462313	0.785754
-39.376362	-13.224153	0.790758
-39.123861	-22.651029	0.795763
-39.349104	-13.643124	0.800768
-39.920770	-14.564057	0.805773
-40.611429	-13.459399	0.810778
-40.841173	-19.991270	0.815782
-40.638576	-17.706096	0.820787
-41.692494	-14.110935	0.825792
-41.906312	-14.100124	0.830797
-42.205319	-7.695840	0.835802
-42.691486	-9.077100	0.840806
-42.494118	-17.402021	0.845811
-42.478962	-4.589491	0.850816
-42.292137	-18.983996	0.855821
-42.340721	-13.425906	0.860826
-43.342228	-17.344372	0.865830
-43.415346	-14.866920	0.870835
-43.752288	-18.710342	0.875840
-43.977465	-17.778475	0.880845
-43.891175	-8.916483	0.885850
-45.093805	-14.143505	0.890854
-45.151312	-16.789218	0.895859
-45.499034	-7.807400	0.900864
-45.663637	-6.324942	0.905869
-45.398625	-10.440914	0.910874
-45.540008	-9.318684	0.915878
-45.612797	-8.616291	0.920883
-46.034330	0.068139	0.925888
-46.886637	-5.930257	0.930893
-47.169303	-9.894556	0.935898
-47.628370	-5.033939	0.940902
-47.283445	-8.837743	0.945907
-47.343049	-6.069292	0.950912
-47.309250	-10.962944	0.955917
-48.111737	-6.817815	0.960922
-48.621996	-10.006795	0.965926
-48.411134	-14.826563	0.970931
-48.727881	-8.680610	0.975936
-48.746417	-14.465628	0.980941
-48.795753	-4.891103	0.985946
-50.236109	-4.157200	0.990950
-50.433026	-11.848906	0.995955
-50.689883	-9.225191	1.000960
-50.719384	-17.243774	1.005965
-50.632064	-19.531830	1.010970
-50.740726	-11.754259	1.015974
-50.342053	-28.319962	1.020979
-50.751014	-20.458330	1.025984
-51.712564	-7.531219	1.030989
-51.895761	-6.617354	1.035994
-52.159989	-5.921146	1.040998
-51.962748	-18.223480	1.046003
-52.180236	-8.159944	1.051008
-52.809652	-14.796914	1.056013
-53.175811	-8.204896	1.061018
-53.480478	-11.722934	1.066022
-53.487852	-15.570811	1.071027
-53.560770	-8.918428	1.076032
-54.111028	-10.895278	1.081037
-54.561348	-4.884082	1.086042
-55.088924	0.306575	1.091046
-55.102508	-7.868963	1.096051
-55.200216	-9.335667	1.101056
-55.000165	-7.691796	1.106061
-55.390706	-10.789502	1.111066
-55.386288	-10.462592	1.116070
-55.792082	-16.963335	1.121075
-56.446048	-3.312431	1.126080
-56.703023	-11.359452	1.131085
-56.580591	-13.823227	1.136090
-56.863422	-9.846640	1.141094
-57.643462	-15.685120	1.146099
-58.077805	-9.587772	1.151104
-58.081845	-8.904264	1.156109
-58.342596	-15.378114	1.161114
-58.317169	-8.228559	1.166118
-57.989962	-11.095455	1.171123
-58.482561	-9.690300	1.176128
-58.696822	-13.768932	1.181133
-59.492061	-9.023534	1.186138
-59.733332	-6.036939	1.191142
-59.896782	-11.071973	1.196147
-60.103093	-10.901578	1.201152
-60.266426	-8.766357	1.206157
-60.893141	0.357177	1.211162
-61.324219	-6.148854	1.216166
-61.317888	-10.955471	1.221171
-61.607420	1.270530	1.226176
-61.674450	-7.701274	1.231181
-61.610306	-17.369277	1.236186
-61.475807	-9.372286	1.241190
-61.651826	-10.692624	1.246195
-62.782833	-6.373899	1.251200
-62.975733	-7.031167	1.256205
-62.931912	-11.781833	1.261210
-63.550017	2.838552	1.266214
-63.362741	-18.342295	1.271219
-64.504405	-2.010967	1.276224
-64.779056	-4.339719	1.281229
-64.662266	-11.360348	1.286234
-64.815975	-9.104966	1.291238
-64.778296	-12.216361	1.296243
-65.108675	-6.452158	1.301248
-64.928161	-5.569715	1.306253
-64.777235	-6.813760	1.311258
-65.897104	-7.838670	1.316262
-65.825633	-11.040909	1.321267
-66.119565	-6.832393	1.326272
-66.391410	-13.407414	1.331277
-67.236418	-13.057838	1.336282
-67.382320	-9.851029	1.341286
-67.666042	-7.372442	1.346291
-68.124938	-6.520267	1.351296
-67.953931	-3.057508	1.356301
-67.917328	-10.288831	1.361306
-68.046123	-4.251751	1.366310
-67.790323	-13.948733	1.371315
-68.918852	-9.489523	1.376320
-69.363424	-8.931970	1.381325
-69.284151	-8.945226	1.386330
-69.670864	-8.849738	1.391334
-69.495432	-20.397804	1.396339
-70.569175	-5.657570	1.401344
-70.942148	-5.613493	1.406349
-71.254884	-19.855801	1.411354
-71.513205	-7.939855	1.416358
-70.740346	-14.967310	1.421363
-71.034390	-1.631161	1.426368
-71.462823	-11.465640	1.431373
-71.405659	-4.811909	1.436378
-72.260609	-10.762498	1.441382
-72.677818	-5.335561	1.446387
-73.050960	-6.304759	1.451392
-72.873505	-10.384524	1.456397
-72.894593	-6.546398	1.461402
-73.070527	-5.743057	1.466406
-73.341519	-6.885656	1.471411
-74.331321	-4.302962	1.476416
-74.469989	-13.963821	1.481421
-74.643329	-7.824054	1.486426
-74.326326	-4.222478	1.491430
-74.284621	-7.366507	1.496435
-74.621517	-8.309739	1.501440
-75.422966	-13.846304	1.506445
-76.192795	-13.306713	1.511450
-76.296107	-7.221562	1.516454
-76.188681	-11.884884	1.521459
-76.066478	-7.316284	1.526464
-76.043171	-10.694460	1.531469
-76.493294	-5.212541	1.536474
-77.474936	-0.590581	1.541478
-77.633896	-3.138390	1.546483
-77.523583	0.599438	1.551488
-77.612690	1.132263	1.556493
-78.114394	-7.536476	1.561498
-78.959456	-1.905481	1.566502
-78.906687	1.181405	1.571507
-79.195149	-1.584716	1.576512
-79.198635	4.011099	1.581517
-79.210985	-6.987682	1.586522
-79.231425	-0.938749	1.591526
-79.386826	-6.321433	1.596531
-80.079017	-0.094947	1.601536
-80.748489	1.417056	1.606541
-80.658805	1.911588	1.611546
-80.953408	1.107772	1.616550
-80.885626	-7.055191	1.621555
-81.208026	0.402385	1.626560
-81.851975	-1.616370	1.631565
-82.467751	2.231051	1.636570
-82.524597	0.521373	1.641574
-82.473848	1.557125	1.646579
-82.743059	-3.859400	1.651584
-82.702047	-5.637774	1.656589
-82.910974	-2.418552	1.661594
-83.450996	-3.151334	1.666598
-83.615694	-1.468171	1.671603
-84.122886	-6.585001	1.676608
-83.858696	-4.756789	1.681613
-84.373991	-3.982690	1.686618
-84.424010	4.724082	1.691622
-84.685215	-4.193067	1.696627
-85.588279	-0.380158	1.701632
-85.630523	3.573953	1.706637
-85.555953	-4.654860	1.711642
-85.700002	-0.081236	1.716646
-85.639031	-1.119761	1.721651
-86.542702	-3.406695	1.726656
-87.199964	-9.177099	1.731661
-87.248236	-5.031763	1.736666
-87.427050	-2.716970	1.741670
-87.551311	-9.916124	1.746675
-87.576793	-0.377321	1.751680
-87.667026	-4.837810	1.756685
-87.340662	-7.152432	1.761690
-88.448064	0.309055	1.766694
-88.816657	-4.306218	1.771699
-89.181239	-4.457902	1.776704
-89.259234	-3.505416	1.781709
-88.923158	0.222057	1.786714
-89.870338	6.394281	1.791718
-90.328840	-1.562731	1.796723
-90.840865	-0.922964	1.801728
-91.081786	-0.954035	1.806733
-90.713003	-2.075506	1.811738
-90.955315	5.749858	1.816742
-90.562226	-6.647668	1.821747
-90.850452	-5.908807	1.826752
-90.975169	-0.915698	1.831757
-92.097038	0.076468	1.836762
-92.256951	-2.603986	1.841766
-92.018196	-2.818098	1.846771
-92.276954	-3.926412	1.851776
-93.124232	-8.564428	1.856781
-93.441573	-6.182885	1.861786
-94.007888	-5.669892	1.866790
-93.746387	-9.372858	1.871795
-94.026804	-8.639434	1.876800
-93.756916	-3.651295	1.881805
-93.976375	-4.576087	1.886810
-94.939484	-3.288363	1.891814
-95.211115	-5.964918	1.896819
-95.167273	-2.773152	1.901824
-95.539929	-0.252603	1.906829
-95.459636	-4.064087	1.911834
-95.475885	-4.361667	1.916838
-96.158747	-8.658492	1.921843
-96.957387	-7.435302	1.926848
-96.847601	-6.112936	1.931853
-96.817795	-4.650439	1.936858
-97.096975	6.990535	1.941862
-97.080544	-8.648746	1.946867
-97.959025	-1.104009	1.951872
-98.382656	-4.694692	1.956877
-98.575452	-4.489435	1.961882
-98.636549	-1.668246	1.966886
-98.427400	-0.791534	1.971891
-98.694442	-13.287123	1.976896
-98.769793	-7.391701	1.981901
-99.262581	-6.795770	1.986906
-99.673918	-5.695134	1.991910
-99.910081	-2.377076	1.996915
-100.226337	-2.051752	2.006912
-100.253645	2.534909	2.016909
-99.443832	-1.960566	2.026906
-99.027105	-6.934298	2.036902
-98.343860	-2.886173	2.046899
-97.711950	-7.393280	2.056896
-97.421692	-4.935241	2.066893
-97.201168	-3.626663	2.076890
-96.189794	-7.143486	2.086886
-95.915641	-10.659136	2.096883
-95.706658	2.064069	2.106880
-94.614014	3.019760	2.116877
-94.357980	0.738064	2.126874
-94.027284	-1.782627	2.136870
-92.947443	-3.156518	2.146867
-92.868708	-0.946388	2.156864
-92.748012	-6.031335	2.166861
-92.311396	3.336126	2.176858
-91.566450	1.882352	2.186854
-90.724023	4.639178	2.196851
-89.989289	-1.159582	2.206848
-89.783206	-7.056519	2.216845
-89.821101	-6.578469	2.226842
-88.961558	-2.240241	2.236838
-88.474555	-3.963283	2.246835
-87.903310	6.749965	2.256832
-87.091238	0.200020	2.266829
-86.886683	-5.296356	2.276826
-86.639152	-5.551000	2.286822
-85.720467	-0.292532	2.296819
-85.468126	-0.795348	2.306816
-85.208435	-1.562565	2.316813
-84.248702	-6.677597	2.326810
-83.945010	-3.751133	2.336806
-83.298647	-5.770863	2.346803
-82.604012	-0.014915	2.356800
-82.197261	-2.283041	2.366797
-82.425558	-2.748146	2.376794
-81.381663	-9.353076	2.386790
-81.209737	-6.335438	2.396787
-80.237188	-3.971622	2.406784
-79.638949	-2.135014	2.416781
-79.367642	-3.217129	2.426778
-78.942995	-5.405035	2.436774
-78.078899	-6.281832	2.446771
-77.846288	-5.658306	2.456768
-77.846960	-3.695443	2.466765
-76.684190	-4.554721	2.476762
-76.237825	-7.016323	2.486758
-75.966064	-13.575572	2.496755
-75.101786	-3.193009	2.506752
-74.874182	-9.688438	2.516749
-74.619888	-4.171552	2.526746
-73.916244	-8.812842	2.536742
-73.043753	-1.262044	2.546739
-73.273570	-5.199458	2.556736
-71.868332	-6.221985	2.566733
-71.604149	-7.686038	2.576730
-71.677451	-8.258612	2.586726
-70.932014	-5.839992	2.596723
-70.085071	-0.815632	2.606720
-69.850541	-7.881452	2.616717
-69.541513	-1.805770	2.626714
-68.670046	-0.345759	2.636710
-68.594751	-5.060421	2.646707
-67.307236	-2.927577	2.656704
-67.141020	-4.670795	2.666701
-67.175142	-3.200900	2.676698
-66.599234	-5.840441	2.686694
-65.621522	-3.494468	2.696691
-65.298737	-5.777535	2.706688
-64.923664	-3.804384	2.716685
-64.155315	-0.235065	2.726682
-63.806190	-3.081462	2.736678
-63.512364	-2.103331	2.746675
-62.822639	4.180198	2.756672
-62.329408	4.648534	2.766669
-61.739529	-3.461297	2.776666
-60.932758	0.128531	2.786662
-60.430857	-1.654867	2.796659
-60.422419	1.537049	2.806656
-60.245274	-7.798216	2.816653
-59.331031	-2.310400	2.826650
-58.970305	-2.568573	2.836646
-58.090249	2.593161	2.846643
-57.273834	0.872869	2.856640
-57.427763	3.786801	2.866637
-56.986350	-1.331502	2.876634
-56.566954	-5.073335	2.886630
-56.247950	-2.242071	2.896627
-54.972473	-0.919107	2.906624
-54.386965	-2.688293	2.916621
-54.429708	-1.273479	2.926618
-54.226433	-3.172012	2.936614
-53.607776	-2.704292	2.946611
-52.839537	3.989662	2.956608
-51.918172	-1.571285	2.966605
-51.401133	0.297150	2.976602
-51.330258	-3.786879	2.986598
-51.184965	-0.033564	2.996595
-50.377392	-4.300647	3.006592
-50.125485	-4.386485	3.016589
-48.698721	0.331827	3.026586
-48.382532	1.694116	3.036582
-48.372044	-0.138110	3.046579
-48.258163	-5.405486	3.056576
-47.362822	-6.365695	3.066573
-46.579566	-4.147756	3.076570
-46.462550	-5.847063	3.086566
-45.363730	2.227208	3.096563
-45.058610	-8.419285	3.106560
-44.994022	-6.172629	3.116557
-44.821907	-4.666547	3.126554
-43.885658	-1.684393	3.136550
-43.307510	-0.559908	3.146547
-42.283256	1.206553	3.156544
-42.086117	-7.046491	3.166541
-41.908701	-0.772368	3.176538
-41.296260	3.103939	3.186534
-40.306241	-3.378650	3.196531
-40.491954	-8.312087	3.206528
-40.311789	-2.680176	3.216525
-39.126539	-2.662135	3.226522
-38.885070	-7.701089	3.236518
-37.726339	-3.953581	3.246515
-37.562379	-6.394691	3.256512
-37.290771	-5.272593	3.266509
-37.121892	-9.086550	3.276506
-36.069210	-2.351180	3.286502
-35.614732	-5.427426	3.296499
-35.572615	2.720479	3.306496
-34.958360	-6.033562	3.316493
-34.025073	-1.040287	3.326490
-33.768848	4.844191	3.336486
-32.735158	1.037579	3.346483
-32.473468	-4.874495	3.356480
-32.089160	1.450528	3.366477
-32.167371	3.172336	3.376474
-31.493501	-5.995837	3.386470
-30.826386	-8.444396	3.396467
-30.653272	-4.911254	3.406464
-29.503918	2.892262	3.416461
-29.441461	-0.901307	3.426458
-28.386330	-3.561521	3.436454
-27.874908	-10.348561	3.446451
-27.725851	-12.268541	3.456448
-27.569434	-7.424817	3.466445
-26.898637	-5.510118	3.476442
-26.269280	-4.788689	3.486438
-25.750402	-8.146093	3.496435
-25.191230	-5.370009	3.506432
-24.740677	-4.695238	3.516429
-24.079411	-5.919381	3.526426
-23.424423	-9.145405	3.536422
-23.094129	-7.648721	3.546419
-22.944821	-8.022441	3.556416
-22.547114	-12.049153	3.566413
-21.773803	-4.507406	3.576410
-20.988818	-6.969753	3.586406
-20.258158	-12.536850	3.596403
-19.836588	-9.839736	3.606400
-19.611630	-15.094088	3.616397
-19.492075	-14.215130	3.626394
-19.250869	-15.293443	3.636390
-18.399612	-9.054441	3.646387
-17.266436	-8.287813	3.656384
-16.782674	-6.387584	3.666381
-16.661861	-6.450921	3.676378
-16.618660	-12.414539	3.686374
-15.539403	-9.278234	3.696371
-15.335750	-8.799086	3.706368
-15.080931	-8.419498	3.716365
-13.793687	-13.258585	3.726362
-13.340900	-16.241880	3.736358
-13.526609	-15.468662	3.746355
-13.113984	-11.029341	3.756352
-11.974855	-8.990458	3.766349
-11.830623	-4.857207	3.776346
-10.593018	-9.955407	3.786342
-10.704082	-8.384252	3.796339
-10.256527	-4.388364	3.806336
-10.016472	-8.822077	3.816333
-9.183376	-5.390912	3.826330
-8.353825	-13.220335	3.836326
-8.317914	-9.094833	3.846323
-7.287684	-3.583927	3.856320
-6.959801	-9.905095	3.866317
-6.813257	-4.471127	3.876314
-6.558377	-11.203236	3.886310
-5.661953	-8.031317	3.896307
-5.514204	-10.818875	3.906304
-4.472012	-2.929836	3.916301
-4.265734	-2.248202	3.926298
-3.893211	-3.886680	3.936294
-3.201335	-0.173882	3.946291
-3.037282	4.333873	3.956288
-2.397018	25.460141	3.966285
-2.098702	35.795397	3.976282
-1.641556	47.372071	3.986278
-1.009388	69.253926	3.996275
-0.841410	80.296419	4.006272
-0.532378	106.076472	4.016269
0.000000	122.700423	4.021274
-0.076743	132.559395	4.026278
0.601329	143.413849	4.031283
0.511308	164.122920	4.036288
0.548778	166.461517	4.041293
1.057930	159.078255	4.046298
0.742130	167.485577	4.051302
0.991171	164.667116	4.056307
0.957557	174.048725	4.061312
0.861775	191.982285	4.066317
1.020322	188.226465	4.071322
1.204923	195.805211	4.076326
1.436112	189.359523	4.081331
1.029905	199.253953	4.086336
1.275783	207.619595	4.091341
1.504190	204.748895	4.096346
1.046799	203.995896	4.101350
1.002724	200.786698	4.106355
1.080008	202.879538	4.111360
1.214488	205.870649	4.116365
1.406089	190.060852	4.121370
1.248722	207.034528	4.126374
1.100431	201.949351	4.131379
1.024265	198.790065	4.136384
1.274723	199.896363	4.141389
1.517734	192.154986	4.146394
1.108933	203.102632	4.151398
1.321129	197.631765	4.156403
1.347492	195.070004	4.161408
0.963575	189.087099	4.166413
1.608551	196.087392	4.171418
1.288827	195.740209	4.176422
1.205749	195.702926	4.181427
1.231527	196.584170	4.186432
1.081879	196.109958	4.191437
0.900511	196.083820	4.196442
1.309578	204.851247	4.201446
1.609366	211.745709	4.206451
1.558473	222.381315	4.211456
1.374486	237.506451	4.216461
1.545797	229.112302	4.221466
1.756870	231.096361	4.226470
1.403309	223.536440	4.231475
1.636761	225.485415	4.236480
1.653272	223.789611	4.241485
1.774916	216.831614	4.246490
1.250024	215.773265	4.251494
1.977789	224.203174	4.256499
1.854473	213.549785	4.261504
1.673019	201.827987	4.266509
1.628335	203.377039	4.271514
1.411890	199.933138	4.276518
1.541827	200.221508	4.281523
1.317881	207.825287	4.286528
1.595858	222.839969	4.291533
1.814640	227.523683	4.296538
1.723877	230.501580	4.301542
2.366332	218.957297	4.306547
1.562614	213.427716	4.311552
1.413548	212.390804	4.316557
1.575351	224.156062	4.321562
1.540051	231.297239	4.326566
1.990141	222.970200	4.331571
1.629375	230.799705	4.336576
1.695614	233.330095	4.341581
1.714711	233.150387	4.346586
1.439075	231.511246	4.351590
1.645809	221.853418	4.356595
1.871267	226.648113	4.361600
1.546817	241.768096	4.366605
1.503840	230.503464	4.371610
1.340272	243.771256	4.376614
2.276705	244.734365	4.381619
1.743674	247.057331	4.386624
1.803191	247.310396	4.391629
2.328366	249.846490	4.396634
1.670229	248.709759	4.401638
2.141118	241.464417	4.406643
2.150000	253.885508	4.411648
2.176184	245.203986	4.416653
2.083715	232.232304	4.421658
1.842503	241.069544	4.426662
2.165129	224.227460	4.431667
1.912847	230.343098	4.436672
2.078884	234.413941	4.441677
2.015549	237.698298	4.446682
2.106077	241.774542	4.451686
1.902136	231.847268	4.456691
2.272417	249.854088	4.461696
2.452967	243.120365	4.466701
2.176892	238.949873	4.471706
1.951053	245.585065	4.476710
2.062738	232.304492	4.481715
2.078439	239.187992	4.486720
1.951196	251.741735	4.491725
2.320521	257.135803	4.496730
2.223636	268.750345	4.501734
2.705518	262.107416	4.506739
2.176952	249.993726	4.511744
1.915350	243.069184	4.516749
2.212848	242.570064	4.521754
2.022170	263.677584	4.526758
2.309084	254.289044	4.531763
2.131240	259.146980	4.536768
2.197923	276.662221	4.541773
2.324633	260.749432	4.546778
2.172428	270.220396	4.551782
2.156085	265.577286	4.556787
2.246730	266.600728	4.561792
2.056885	271.107621	4.566797
2.362583	261.698797	4.571802
2.150172	273.553489	4.576806
1.977147	271.108797	4.581811
2.316423	271.222789	4.586816
2.171959	276.954139	4.591821
2.489001	276.881185	4.596826
2.524937	296.565530	4.601830
2.777125	285.467077	4.606835
2.516691	278.368670	4.611840
2.536845	279.463381	4.616845
2.563861	267.922701	4.621850
2.531886	276.738929	4.626854
2.258046	268.222518	4.631859
2.428341	285.655293	4.636864
2.574382	293.500758	4.641869
2.705949	296.113681	4.646874
2.637617	288.433876	4.651878
2.510206	278.872193	4.656883
2.626483	273.973868	4.661888
2.250644	287.383410	4.666893
2.658185	288.882253	4.671898
2.641961	304.190429	4.676902
2.765923	293.719027	4.681907
2.597503	300.275667	4.686912
2.702588	302.109550	4.691917
3.094445	305.003793	4.696922
2.548257	301.692618	4.701926
2.787501	300.620013	4.706931
2.702556	300.854179	4.711936
3.049234	299.660972	4.716941
2.786156	292.094717	4.721946
2.242681	285.952699	4.726950
2.513765	295.435677	4.731955
2.837286	291.300072	4.736960
2.907660	298.751359	4.741965
2.708235	298.917062	4.746970
2.774026	306.601180	4.751974
2.698282	310.790620	4.756979
2.336649	306.509757	4.761984
2.691886	303.211722	4.766989
2.666014	298.946106	4.771994
2.600885	314.213254	4.776998
2.569005	311.061017	4.782003
2.696364	314.618106	4.787008
2.710948	335.975308	4.792013
3.257562	335.113867	4.797018
2.894929	337.140053	4.802022
2.957318	338.154563	4.807027
2.962110	336.000102	4.812032
2.668005	345.404623	4.817037
3.091563	338.295146	4.822042
3.115748	345.745619	4.827046
3.124344	334.952492	4.832051
2.831795	330.174340	4.837056
3.005624	339.058745	4.842061
3.104651	338.567426	4.847066
2.867227	337.827132	4.852070
3.288885	337.751458	4.857075
3.240930	342.977060	4.862080
2.976345	344.721988	4.867085
3.251791	344.404121	4.872090
3.027824	348.520631	4.877094
3.018367	338.556347	4.882099
3.264415	342.834000	4.887104
2.999983	345.945462	4.892109
2.987782	342.375553	4.897114
2.976433	345.185411	4.902118
3.117568	343.528158	4.907123
2.955183	334.867550	4.912128
2.946131	338.989910	4.917133
3.039828	346.573521	4.922138
3.147722	343.193691	4.927142
3.144207	364.491176	4.932147
3.407578	370.004063	4.937152
2.964362	372.053860	4.942157
3.540416	368.450076	4.947162
3.342496	374.643993	4.952166
3.364329	367.761854	4.957171
3.239170	373.960495	4.962176
3.372602	371.192913	4.967181
3.779402	366.148375	4.972186
3.713015	376.930511	4.977190
3.583175	358.584702	4.982195
3.265305	342.320384	4.987200
2.964885	344.675492	4.992205
3.319964	357.917094	4.997210
3.186947	375.063341	5.002214
3.635680	371.993718	5.007219
3.408210	367.356727	5.012224
3.393861	376.628706	5.017229
3.474587	361.682883	5.022234
3.505346	368.439230	5.027238
3.702082	372.016221	5.032243
3.499355	373.989293	5.037248
3.664470	371.790519	5.042253
4.025476	367.105613	5.047258
3.743475	374.785393	5.052262
3.702217	364.111602	5.057267
3.776684	373.990090	5.062272
3.940730	362.225364	5.067277
3.667963	336.741680	5.072282
3.406264	344.978520	5.077286
3.580341	337.510155	5.082291
3.315413	354.155279	5.087296
3.147159	359.181368	5.092301
3.447659	363.084739	5.097306
3.521693	377.132251	5.102310
3.611863	373.124264	5.107315
3.412854	377.132651	5.112320
3.326072	379.191705	5.117325
3.679373	366.686801	5.122330
3.473142	381.318075	5.127334
3.977568	387.499691	5.132339
3.711431	396.069215	5.137344
3.789760	405.208843	5.142349
4.129344	396.871595	5.147354
3.704189	389.766865	5.152358
3.751913	382.962722	5.157363
3.887610	380.597134	5.162368
3.878015	401.840620	5.167373
3.948005	397.409916	5.172378
3.514933	408.693647	5.177382
3.776012	403.619354	5.182387
3.694337	414.558169	5.187392
3.619164	409.572312	5.192397
3.856775	407.141496	5.197402
4.036352	419.141159	5.202406
3.887149	412.557479	5.207411
3.864600	414.440729	5.212416
3.554692	412.634376	5.217421
4.139907	406.020256	5.222426
3.619777	412.434884	5.227430
3.804264	407.727889	5.232435
3.718626	407.733456	5.237440
3.481780	422.733533	5.242445
4.098047	428.508285	5.247450
4.392734	426.521695	5.252454
4.413957	422.482290	5.257459
4.226388	425.773445	5.262464
3.958023	432.604612	5.267469
4.526299	428.009097	5.272474
4.448331	437.803740	5.277478
4.306449	415.332330	5.282483
4.121623	410.952500	5.287488
3.971215	410.987540	5.292493
4.287373	409.384377	5.297498
4.003200	409.489125	5.302502
3.822573	416.324898	5.307507
3.956885	418.295249	5.312512
3.851336	429.294663	5.317517
4.633335	429.388233	5.322522
4.385787	429.285039	5.327526
4.206309	426.070391	5.332531
4.248196	433.542643	5.337536
4.060656	444.778835	5.342541
4.098812	435.214305	5.347546
4.101439	443.053008	5.352550
4.384355	437.490424	5.357555
3.968008	440.366575	5.362560
4.213253	441.389687	5.367565
4.618826	437.888121	5.372570
4.438305	438.170083	5.377574
4.657012	441.375219	5.382579
4.700914	441.000574	5.387584
4.693115	437.152259	5.392589
4.718981	439.180235	5.397594
4.644408	437.438710	5.402598
4.593117	435.893430	5.407603
4.306702	433.643318	5.412608
4.751169	443.432559	5.417613
4.497222	439.602901	5.422618
4.268632	437.938582	5.427622
4.356606	423.196732	5.432627
4.310081	441.913553	5.437632
4.364746	440.251467	5.442637
4.570594	437.693097	5.447642
4.510750	445.911957	5.452646
4.632989	440.930303	5.457651
4.331203	442.475381	5.462656
4.277385	449.233336	5.467661
4.575126	444.536979	5.472666
4.371321	444.945937	5.477670
4.664307	459.918108	5.482675
4.935219	466.153421	5.487680
4.614476	463.185348	5.492685
4.796324	446.499735	5.497690
4.360655	455.004023	5.502694
4.617306	460.156925	5.507699
4.881977	468.818368	5.512704
4.918103	478.946985	5.517709
4.982219	468.078661	5.522714
4.590223	455.149484	5.527718
4.793147	468.527282	5.532723
4.439341	471.234421	5.537728
4.743081	469.913332	5.542733
4.881478	476.241240	5.547738
4.580261	471.810019	5.552742
4.834067	469.450317	5.557747
4.721431	469.136916	5.562752
4.887863	474.850800	5.567757
4.619856	474.428345	5.572762
4.456388	471.241624	5.577766
4.701605	464.638983	5.582771
4.642693	474.640462	5.587776
4.742630	474.049332	5.592781
4.947437	471.791479	5.597786
4.995897	481.128503	5.602790
5.156840	476.625290	5.607795
4.993267	478.710887	5.612800
4.910166	471.675775	5.617805
5.221583	470.547201	5.622810
4.964885	468.327881	5.627814
4.945617	465.877629	5.632819
4.799396	480.020513	5.637824
4.859622	490.065422	5.642829
5.125598	495.151078	5.647834
4.714322	505.361692	5.652838
5.353757	502.245468	5.657843
5.207009	502.485134	5.662848
5.300636	507.301154	5.667853
5.602631	499.358834	5.672858
5.116246	492.985075	5.677862
5.156830	477.825952	5.682867
5.319360	478.267985	5.687872
4.970151	478.482764	5.692877
5.278662	477.922415	5.697882
5.244290	490.369210	5.702886
5.216494	480.068844	5.707891
5.228634	468.699991	5.712896
4.698059	482.627092	5.717901
5.045390	501.860718	5.722906
5.349045	507.061306	5.727910
5.132362	507.167114	5.732915
5.390662	503.112702	5.737920
5.250800	505.701538	5.742925
5.701122	503.110372	5.747930
5.586009	507.826964	5.752934
5.676472	501.777619	5.757939
5.169731	487.260484	5.762944
5.397811	512.056333	5.767949
5.595020	499.901003	5.772954
5.046351	510.883273	5.777958
5.156634	503.564714	5.782963
5.373798	507.829436	5.787968
5.118230	509.650838	5.792973
5.444212	501.793347	5.797978
5.331265	506.424724	5.802982
5.243147	507.629340	5.807987
5.290608	513.047985	5.812992
5.122478	503.822067	5.817997
5.308256	507.387880	5.823002
5.196297	518.830656	5.828006
5.590665	531.031054	5.833011
5.255976	522.347959	5.838016
4.871226	538.065892	5.843021
5.582988	539.129375	5.848026
5.743971	542.875131	5.853030
5.618221	533.348931	5.858035
5.589480	537.903028	5.863040
5.676131	536.032573	5.868045
5.912127	537.331131	5.873050
5.743995	537.374828	5.878054
5.709375	547.959812	5.883059
6.137669	541.036734	5.888064
5.899358	544.829665	5.893069
5.650252	522.476893	5.898074
5.363338	521.938375	5.903078
5.511796	536.670907	5.908083
5.684554	540.151857	5.913088
5.599477	538.347135	5.918093
5.872587	533.584182	5.923098
5.805432	545.209992	5.928102
5.540031	548.505773	5.933107
5.863411	540.438724	5.938112
5.875408	547.820665	5.943117
6.312093	539.048901	5.948122
5.722999	541.291798	5.953126
6.082096	539.825372	5.958131
5.828848	544.520646	5.963136
5.730763	547.724783	5.968141
6.068435	541.012274	5.973146
5.680563	547.396769	5.978150
6.017049	544.077713	5.983155
6.008808	540.579920	5.988160
5.472857	544.752879	5.993165
5.896466	541.092010	5.998170
5.587519	550.287565	6.003174
5.484501	536.039996	6.008179
5.709354	539.841678	6.013184
5.427720	537.694362	6.018189
5.819814	545.671094	6.023194
5.605164	571.138289	6.028198
5.829162	571.121592	6.033203
6.072727	567.984078	6.038208
5.912502	572.025364	6.043213
6.001516	560.821518	6.048218
5.750250	570.183757	6.053222
6.083392	575.127482	6.058227
6.024082	574.228029	6.063232
5.932698	568.556286	6.068237
6.306398	568.614654	6.073242
6.223355	569.478812	6.078246
5.915698	563.936225	6.083251
5.986663	567.937451	6.088256
6.044389	570.266046	6.093261
6.258164	569.123046	6.098266
6.182923	565.517346	6.103270
6.351789	570.422163	6.108275
6.463368	572.325848	6.113280
5.775589	558.553389	6.118285
6.107139	550.572206	6.123290
6.143392	553.797908	6.128294
5.936989	553.665799	6.133299
5.701869	542.399406	6.138304
5.929872	566.993083	6.143309
6.229141	565.739230	6.148314
5.691073	570.880894	6.153318
6.286597	571.985927	6.158323
6.294388	568.483894	6.163328
5.927372	564.997749	6.168333
6.062903	549.465648	6.173338
5.859239	551.256161	6.178342
5.991075	558.897301	6.183347
6.086331	556.771639	6.188352
5.864106	569.109098	6.193357
6.175086	570.562784	6.198362
5.899229	571.484328	6.203366
5.702889	566.971972	6.208371
6.128065	567.967469	6.213376
5.854599	566.545401	6.218381
6.007067	568.491452	6.223386
5.884887	577.204779	6.228390
6.022177	568.595060	6.233395
6.265746	561.936212	6.238400
5.978789	572.964781	6.243405
6.349150	568.813256	6.248410
6.100738	573.531221	6.253414
6.019543	551.783274	6.258419
6.008776	545.720087	6.263424
5.774271	551.417507	6.268429
6.101964	554.711578	6.273434
6.393929	564.203696	6.278438
6.043663	550.997766	6.283443
6.278729	543.480130	6.288448
6.129819	551.789178	6.293453
5.980019	542.272283	6.298458
6.028981	540.303676	6.303462
6.088796	546.497015	6.308467
6.248071	542.605417	6.313472
5.915136	546.920392	6.318477
5.581780	533.021382	6.323482
5.657287	542.922105	6.328486
5.766797	547.001602	6.333491
6.277374	551.862853	6.338496
5.911989	564.441285	6.343501
6.321314	562.291046	6.348506
6.081639	555.688343	6.353510
5.887441	544.094299	6.358515
6.310529	549.213356	6.363520
5.836254	547.497156	6.368525
5.819830	548.089793	6.373530
6.042814	553.124767	6.378534
5.805758	539.358797	6.383539
6.489513	550.586360	6.388544
6.419866	546.174987	6.393549
6.176729	542.578939	6.398554
6.208804	545.744551	6.403558
6.102386	535.689632	6.408563
6.318409	542.004713	6.413568
6.027697	543.703865	6.418573
6.182455	542.500190	6.423578
5.968164	546.970953	6.428582
5.887971	542.878057	6.433587
6.013237	541.939360	6.438592
6.126277	537.794931	6.443597
6.050479	543.023238	6.448602
6.166069	547.157970	6.453606
5.890833	544.901648	6.458611
5.871337	543.117048	6.463616
5.757995	549.624809	6.468621
5.739996	542.056724	6.473626
6.216696	542.961003	6.478630
6.073099	544.497459	6.483635
5.997101	541.720322	6.488640
5.998818	552.213645	6.493645
6.266422	544.291008	6.498650
6.223409	548.099160	6.503654
5.919901	544.578625	6.508659
6.061399	540.138013	6.513664
6.067799	546.733298	6.518669
6.366929	537.700538	6.523674
6.008665	545.240289	6.528678
5.880430	541.077203	6.533683
6.111613	542.639020	6.538688
5.924419	544.401150	6.543693
6.102494	542.062068	6.548698
6.067202	545.676929	6.553702
6.033355	546.461108	6.558707
6.492181	549.523494	6.563712
5.902485	549.161410	6.568717
5.977373	541.785150	6.573722
6.035258	540.996932	6.578726
5.817810	545.777054	6.583731
5.840208	552.738520	6.588736
5.648658	547.038970	6.593741
6.486981	541.698544	6.598746
6.169894	544.052890	6.603750
6.214008	542.399447	6.608755
6.120301	538.011399	6.613760
6.196943	535.966969	6.618765
6.056907	521.562343	6.623770
5.815267	507.391036	6.628774
6.059472	513.508638	6.633779
5.870195	509.798892	6.638784
5.958939	532.239514	6.643789
6.249590	529.661562	6.648794
5.775347	529.175967	6.653798
6.283110	538.301595	6.658803
6.241792	521.644962	6.663808
6.069513	526.693084	6.668813
5.652440	523.953682	6.673818
5.740936	517.370656	6.678822
5.812872	536.516133	6.683827
6.363275	544.949343	6.688832
5.932933	550.168871	6.693837
6.412661	539.775741	6.698842
6.088809	518.825017	6.703846
5.687889	513.660009	6.708851
6.053628	519.387675	6.713856
5.996624	534.487534	6.718861
5.902829	525.759417	6.723866
6.138157	531.904940	6.728870
5.810740	524.345277	6.733875
5.962345	533.032385	6.738880
6.340814	539.285636	6.743885
6.265058	529.749976	6.748890
5.971321	520.693049	6.753894
5.799720	513.528318	6.758899
5.966362	517.647484	6.763904
6.004754	523.705237	6.768909
6.282446	522.547316	6.773914
5.811354	517.287955	6.778918
6.078514	517.706151	6.783923
5.856517	513.399148	6.788928
5.883597	527.009374	6.793933
6.401528	531.274027	6.798938
6.191915	518.429251	6.803942
5.866807	512.163561	6.808947
6.205866	499.834961	6.813952
6.151838	505.951229	6.818957
5.916683	504.643595	6.823962
5.757560	512.129633	6.828966
6.093671	510.976642	6.833971
5.843985	505.801197	6.838976
5.501199	513.539261	6.843981
6.020615	528.335866	6.848986
6.146915	537.015918	6.853990
6.259235	542.270500	6.858995
6.143150	527.048074	6.864000
5.722101	515.633503	6.869005
5.790325	534.332223	6.874010
5.924538	539.969964	6.879014
6.248672	544.822026	6.884019
6.502240	533.878475	6.889024
5.762237	525.734530	6.894029
5.921064	521.241324	6.899034
6.496568	523.279729	6.904038
5.684951	515.627578	6.909043
6.177884	514.944926	6.914048
5.659897	517.144273	6.919053
5.779669	534.117803	6.924058
5.937026	541.438768	6.929062
5.654282	545.446659	6.934067
5.924657	533.003898	6.939072
5.782872	542.980466	6.944077
6.204291	541.361636	6.949082
6.106251	542.578554	6.954086
5.983474	545.166737	6.959091
6.262112	539.698957	6.964096
6.038306	540.049856	6.969101
5.988094	533.992811	6.974106
6.136893	537.345115	6.979110
6.140150	539.434274	6.984115
6.257540	537.646544	6.989120
5.852971	540.568124	6.994125
6.066505	542.985173	6.999130
6.155295	540.111483	7.004134
5.924020	541.232454	7.009139
6.521070	532.676472	7.014144
6.033477	535.800653	7.019149
6.359481	516.727163	7.024154
5.856499	513.768339	7.029158
5.652565	508.937962	7.034163
6.169994	508.529306	7.039168
5.907108	510.569979	7.044173
5.884998	506.354202	7.049178
5.921329	522.884499	7.054182
5.836177	524.069089	7.059187
6.453123	536.498253	7.064192
6.221578	517.895189	7.069197
6.539617	507.376508	7.074202
6.127312	514.667468	7.079206
6.008813	515.246616	7.084211
6.272404	512.764516	7.089216
6.114453	511.762800	7.094221
6.130840	506.421340	7.099226
6.273613	509.316612	7.104230
6.049606	507.735790	7.109235
6.220081	514.994777	7.114240
5.991449	513.071153	7.119245
6.053109	507.522094	7.124250
6.029955	518.310194	7.129254
5.916694	510.633575	7.134259
6.178904	509.285023	7.139264
5.843312	515.070606	7.144269
5.991513	513.257056	7.149274
5.953026	512.124061	7.154278
6.091919	517.382326	7.159283
6.159300	510.516460	7.164288
5.985513	508.901470	7.169293
5.786435	509.495343	7.174298
6.029280	511.281574	7.179302
5.978617	507.507237	7.184307
5.984064	506.278560	7.189312
5.654983	516.259681	7.194317
5.859394	499.902988	7.199322
5.932532	504.765421	7.204326
6.047824	515.104340	7.209331
5.899669	505.333023	7.214336
5.977984	513.216456	7.219341
5.998376	515.228180	7.224346
5.985796	515.747163	7.229350
5.852012	509.127144	7.234355
5.929597	502.777607	7.239360
5.643230	512.594176	7.244365
5.663913	507.455264	7.249370
5.748143	522.993696	7.254374
6.099335	533.824408	7.259379
6.061762	543.771485	7.264384
6.116000	550.426340	7.269389
6.311169	538.166530	7.274394
5.930805	526.143327	7.279398
5.895054	517.670827	7.284403
5.856524	520.119154	7.289408
5.960003	535.573304	7.294413
5.814946	547.631757	7.299418
6.128163	542.179563	7.304422
6.222854	547.621973	7.309427
6.299092	545.870460	7.314432
5.814904	528.495625	7.319437
5.910463	524.633725	7.324442
5.873551	527.186375	7.329446
6.221999	539.617969	7.334451
6.185685	534.554397	7.339456
5.855514	523.498532	7.344461
5.866156	531.016262	7.349466
6.350926	543.980994	7.354470
6.105051	531.431906	7.359475
6.421736	522.324812	7.364480
6.129546	527.221500	7.369485
6.309405	519.623820	7.374490
6.116879	514.444432	7.379494
6.094376	508.268549	7.384499
6.200408	514.101972	7.389504
6.207538	520.229825	7.394509
6.357359	509.889963	7.399514
6.088592	512.532706	7.404518
5.923638	507.760602	7.409523
6.276645	505.936228	7.414528
5.915176	515.776484	7.419533
6.015241	512.756085	7.424538
5.589851	515.906666	7.429542
5.641487	510.526215	7.434547
5.785436	507.804820	7.439552
5.691779	517.721699	7.444557
5.928950	510.848832	7.449562
5.874866	514.813128	7.454566
5.930804	514.099039	7.459571
6.069893	506.916608	7.464576
6.017429	515.775636	7.469581
5.952981	516.909633	7.474586
5.875869	504.313479	7.479590
5.888900	514.922519	7.484595
5.781950	512.384360	7.489600
5.765453	524.271133	7.494605
5.997383	528.535389	7.499610
5.981132	541.966711	7.504614
5.975565	545.602304	7.509619
6.170313	542.928931	7.514624
5.540153	549.871564	7.519629
5.873807	549.246466	7.524634
5.900066	541.410170	7.529638
5.846942	547.754823	7.534643
6.259743	533.627272	7.539648
6.174206	539.869542	7.544653
6.244025	544.328188	7.549658
6.330318	540.123855	7.554662
6.190253	542.699311	7.559667
6.142671	528.823631	7.564672
5.766376	523.419709	7.569677
6.149068	532.540981	7.574682
6.059336	532.995187	7.579686
5.610793	522.652375	7.584691
6.085895	534.285870	7.589696
6.214127	542.276298	7.594701
6.044489	536.611407	7.599706
6.076957	525.440236	7.604710
6.030941	529.962460	7.609715
6.013399	523.620576	7.614720
6.176739	521.876547	7.619725
5.954863	513.232992	7.624730
5.710193	520.590326	7.629734
6.037970	530.147141	7.634739
6.297277	535.434215	7.639744
6.246082	528.950094	7.644749
6.041862	515.922874	7.649754
6.209148	512.674665	7.654758
5.925011	516.236398	7.659763
6.208642	507.997355	7.664768
5.834319	511.428581	7.669773
5.769647	511.941391	7.674778
5.778252	508.485414	7.679782
6.010886	513.599687	7.684787
6.186879	511.859879	7.689792
5.932575	512.401919	7.694797
5.988301	509.133308	7.699802
6.050168	516.691686	7.704806
5.811630	517.633687	7.709811
5.819752	509.475590	7.714816
5.786865	540.124365	7.719821
6.124814	539.703790	7.724826
5.880707	539.176337	7.729830
5.827398	544.842370	7.734835
6.183342	546.237299	7.739840
5.784045	548.201107	7.744845
6.236767	542.932624	7.749850
6.078748	551.940382	7.754854
5.936387	543.934863	7.759859
6.319998	541.438212	7.764864
6.146071	542.272820	7.769869
6.055744	540.752347	7.774874
6.171679	539.890973	7.779878
6.066996	526.887716	7.784883
6.034351	519.459613	7.789888
5.581314	513.690300	7.794893
6.121469	526.782799	7.799898
6.199794	534.970342	7.804902
5.965421	536.952424	7.809907
5.801266	530.970094	7.814912
5.988807	540.174403	7.819917
5.799450	539.141378	7.824922
5.999704	535.155180	7.829926
6.196831	547.093032	7.834931
6.131815	539.817889	7.839936
6.072190	543.550052	7.844941
6.243889	535.213889	7.849946
5.813142	526.028485	7.854950
5.796834	538.907066	7.859955
6.103767	534.988454	7.864960
6.064512	541.729830	7.869965
6.130485	547.542073	7.874970
5.992208	539.100747	7.879974
5.911508	545.684603	7.884979
6.121964	539.982031	7.889984
6.026292	536.333740	7.894989
6.334659	532.480014	7.899994
5.927223	511.942555	7.904998
5.558367	514.760138	7.910003
6.004966	523.881085	7.915008
5.987791	538.713076	7.920013
6.286317	541.779902	7.925018
5.910025	535.092872	7.930022
6.058672	539.952482	7.935027
6.236827	534.296899	7.940032
6.144620	528.915593	7.945037
5.817987	519.848129	7.950042
6.204706	519.352383	7.955046
6.036695	527.521708	7.960051
5.684886	506.109317	7.965056
5.682528	529.808850	7.970061
6.062425	532.938176	7.975066
6.155160	538.786439	7.980070
5.884507	539.813091	7.985075
5.909576	538.894142	7.990080
5.297181	538.415637	7.995085
5.921884	532.376682	8.000090
6.327429	543.942766	8.005094
5.874303	546.614464	8.010099
6.356815	537.115810	8.015104
5.989296	544.298330	8.020109
6.138054	541.393513	8.025126
6.099068	541.810835	8.030144
5.931805	542.465722	8.035162
5.867685	539.844709	8.040179
5.657652	545.695084	8.045197
6.090157	548.606392	8.050214
6.246227	553.429878	8.055232
5.996841	546.548903	8.060250
6.295518	544.403602	8.065267
5.432693	554.069094	8.070285
5.701489	543.646459	8.075302
5.833725	545.056418	8.080320
5.889352	547.470724	8.085338
6.184901	539.545451	8.090355
6.145767	550.385869	8.095373
6.029337	541.595613	8.100390
6.101799	538.266009	8.105408
6.184534	542.320196	8.110426
6.140303	547.815188	8.115443
6.325806	542.468385	8.120461
6.311675	539.012973	8.125478
6.362980	546.700647	8.130496
6.170860	546.130014	8.135514
6.160088	537.904703	8.140531
5.736599	540.770366	8.145549
6.086028	545.241184	8.150566
6.154453	541.332762	8.155584
5.761047	538.144667	8.160602
6.431730	541.008660	8.165619
6.070036	536.627998	8.170637
6.177554	539.151025	8.175654
6.513668	539.252512	8.180672
6.200912	549.654415	8.185690
6.247340	542.738237	8.190707
6.310688	544.610752	8.195725
6.055926	546.195416	8.200742
6.322076	545.200694	8.205760
6.103642	549.754721	8.210778
6.301319	532.337679	8.215795
6.225771	543.526223	8.220813
6.216695	531.455636	8.225830
6.397763	538.565756	8.230848
5.862194	545.498310	8.235866
6.132880	535.400541	8.240883
5.771880	543.355881	8.245901
6.014854	541.776064	8.250918
6.274004	550.113328	8.255936
6.409361	571.020605	8.260954
6.320177	559.518143	8.265971
6.238413	549.522622	8.270989
6.206986	553.468165	8.276006
6.489953	535.919091	8.281024
6.036849	548.910780	8.286042
6.407880	537.864570	8.291059
6.032059	551.381812	8.296077
6.165715	560.522483	8.301094
6.197176	572.457054	8.306112
6.302845	573.639542	8.311130
6.477591	570.885669	8.316147
6.465339	572.871289	8.321165
6.476873	574.197899	8.326182
6.312610	569.669189	8.331200
6.382074	578.531545	8.336218
6.512988	566.964681	8.341235
6.102823	547.091369	8.346253
6.213302	565.848385	8.351270
6.525925	563.291549	8.356288
6.400972	573.153153	8.361306
6.473949	576.055304	8.366323
6.481486	554.750312	8.371341
6.415302	555.893740	8.376358
6.228923	541.843593	8.381376
6.164505	547.960387	8.386394
6.406431	556.577062	8.391411
6.642889	567.102190	8.396429
6.111449	563.951512	8.401446
6.748321	563.540435	8.406464
6.188737	563.825869	8.411482
6.533768	555.517027	8.416499
6.333737	568.524499	8.421517
6.454346	579.902028	8.426534
6.644085	570.368783	8.431552
6.442075	574.263057	8.436570
6.322336	552.000275	8.441587
6.139323	568.229700	8.446605
6.072539	571.557918	8.451622
6.782510	569.084879	8.456640
6.639260	576.705973	8.461658
6.684969	574.066964	8.466675
6.421839	575.897094	8.471693
6.436957	578.488574	8.476710
6.534084	567.112331	8.481728
6.621571	578.949053	8.486746
6.751854	569.931327	8.491763
6.422510	552.871592	8.496781
6.526113	553.996353	8.501798
6.756708	557.785919	8.506816
6.394701	540.808962	8.511834
6.519885	541.110720	8.516851
6.420459	543.850679	8.521869
6.246452	558.867076	8.526886
6.327921	563.247045	8.531904
6.479086	576.140861	8.536922
6.709737	576.657816	8.541939
6.437006	580.604350	8.546957
6.298520	582.600443	8.551974
6.425340	565.441734	8.556992
6.693234	578.381179	8.562010
6.504970	571.010184	8.567027
6.773207	565.899656	8.572045
6.193773	574.267142	8.577063
6.505556	569.157275	8.582080
6.418015	581.622940	8.587098
6.630423	571.849736	8.592115
6.609680	564.387426	8.597133
6.177677	576.964060	8.602151
6.893505	566.255589	8.607168
6.643346	570.107248	8.612186
6.335553	567.571458	8.617203
6.711764	571.627052	8.622221
6.666344	583.704471	8.627239
6.853160	569.674975	8.632256
6.894428	576.952741	8.637274
6.562627	575.408455	8.642291
6.798695	567.400701	8.647309
6.698239	572.020231	8.652327
7.037866	568.394234	8.657344
6.891578	570.418386	8.662362
6.895831	568.113976	8.667379
6.809166	579.571297	8.672397
6.880691	577.022691	8.677415
6.734577	565.714285	8.682432
6.676129	574.579711	8.687450
6.710713	589.115171	8.692467
6.851074	581.721641	8.697485
6.872543	570.547872	8.702503
6.991923	579.005730	8.707520
6.664918	578.802093	8.712538
6.788609	582.959146	8.717555
6.898635	570.846563	8.722573
6.876927	569.309194	8.727591
6.931469	571.137110	8.732608
6.795396	578.720995	8.737626
7.018909	577.940797	8.742643
6.851272	556.210511	8.747661
6.648447	552.095839	8.752679
6.612794	543.636277	8.757696
6.545879	552.262951	8.762714
6.803456	571.909135	8.767731
6.702840	574.222161	8.772749
6.468516	571.932061	8.777767
7.105462	571.728240	8.782784
6.702526	580.745589	8.787802
6.744604	577.870189	8.792819
7.094066	569.542300	8.797837
7.000424	570.212554	8.802855
6.763271	576.672311	8.807872
6.867298	582.254765	8.812890
6.595588	576.365397	8.817907
6.901924	570.586007	8.822925
6.604096	580.043792	8.827943
6.817377	567.673383	8.832960
6.579392	572.204671	8.837978
6.503814	585.988344	8.842995
6.598664	578.381305	8.848013
6.682306	578.830287	8.853031
6.686138	576.846986	8.858048
6.776244	586.945409	8.863066
7.246877	598.074257	8.868083
7.338028	599.578420	8.873101
6.641339	590.842886	8.878119
6.901912	581.086699	8.883136
6.879979	585.945969	8.888154
6.958356	594.373620	8.893171
7.045533	590.423107	8.898189
7.022748	599.124779	8.903207
7.174944	593.244141	8.908224
6.722188	582.118381	8.913242
6.693839	594.787232	8.918259
7.031251	598.660294	8.923277
6.850218	600.095756	8.928295
7.334159	602.854276	8.933312
6.846988	606.896361	8.938330
7.254667	602.482171	8.943347
7.199295	598.081474	8.948365
6.982648	602.795445	8.953383
7.254399	595.866930	8.958400
7.406320	590.721525	8.963418
7.042711	583.183707	8.968435
7.136652	576.316335	8.973453
6.682164	590.446595	8.978471
7.025460	571.380902	8.983488
6.864714	591.165469	8.988506
7.155938	600.952271	8.993523
7.260964	595.141251	8.998541
7.000982	600.487354	9.003559
7.277937	594.280370	9.008576
7.162350	580.706620	9.013594
6.715572	580.604896	9.018611
7.311850	586.238901	9.023629
6.994564	606.052755	9.028647
7.395008	599.533017	9.033664
7.333834	593.084407	9.038682
6.856883	587.060331	9.043699
7.118958	588.099606	9.048717
7.248580	607.496372	9.053735
7.555808	594.629512	9.058752
7.254429	591.297042	9.063770
7.317545	577.584065	9.068787
7.035019	575.012203	9.073805
7.031164	570.013654	9.078823
7.223068	567.719506	9.083840
7.152993	576.670120	9.088858
7.098335	579.156627	9.093875
7.295436	567.394761	9.098893
6.678855	580.086995	9.103911
7.073253	594.519574	9.108928
7.419995	606.570061	9.113946
7.105293	609.718096	9.118963
7.317878	601.591780	9.123981
7.044699	602.707485	9.128999
7.126430	611.790845	9.134016
7.288757	601.079916	9.139034
7.177188	615.205576	9.144051
6.983136	609.272630	9.149069
7.441924	614.122380	9.154087
7.382371	603.305878	9.159104
7.347348	600.266285	9.164122
7.264150	616.031427	9.169139
7.255984	607.364142	9.174157
7.202558	612.446338	9.179175
7.287107	608.972010	9.184192
7.273671	611.793996	9.189210
7.401897	610.994735	9.194227
7.496736	604.042562	9.199245
7.542877	621.786944	9.204263
7.144895	615.964334	9.209280
7.128555	611.393007	9.214298
7.164980	613.576661	9.219315
7.928118	603.868334	9.224333
7.249965	615.494881	9.229351
7.539457	603.362791	9.234368
7.426641	608.859123	9.239386
7.152078	611.115531	9.244403
7.311698	604.186487	9.249421
7.419756	615.455892	9.254439
7.377423	615.843064	9.259456
7.353194	605.055748	9.264474
7.250056	616.608732	9.269491
7.139957	616.075494	9.274509
7.257934	620.285469	9.279527
7.195195	617.801409	9.284544
7.294028	610.855264	9.289562
7.253955	620.249133	9.294579
7.359225	626.498085	9.299597
7.451728	625.954329	9.304615
7.721949	633.777635	9.309632
7.559092	622.334961	9.314650
7.325790	635.389531	9.319667
7.647995	619.910893	9.324685
7.691799	619.840131	9.329703
7.212212	619.402918	9.334720
7.673907	614.748889	9.339738
7.518095	624.826252	9.344755
7.509965	607.179247	9.349773
7.591630	609.986469	9.354791
7.287478	616.594335	9.359808
7.692704	623.547108	9.364826
7.907711	640.120121	9.369843
7.760324	621.176956	9.374861
7.581692	618.017251	9.379879
7.262513	616.790929	9.384896
7.428958	613.547511	9.389914
7.611154	620.226409	9.394931
7.759157	626.436791	9.399949
7.543881	612.497262	9.404967
7.429934	613.649588	9.409984
7.612491	619.463130	9.415002
7.906626	632.810453	9.420019
7.808950	620.147421	9.425037
7.501220	607.630790	9.430055
7.471024	601.741968	9.435072
7.639082	619.641739	9.440090
7.612521	629.281784	9.445107
7.942559	628.393006	9.450125
7.783220	616.401365	9.455143
7.685500	617.193942	9.460160
7.898379	614.678219	9.465178
7.382137	624.514695	9.470195
7.823081	615.282912	9.475213
7.742737	613.972949	9.480231
7.900030	616.946377	9.485248
7.690484	610.899862	9.490266
7.550913	616.771074	9.495283
7.744597	611.144173	9.500301
7.760579	613.700872	9.505319
7.509871	614.557755	9.510336
7.663666	608.486309	9.515354
7.479170	616.761846	9.520371
8.064046	633.937340	9.525389
8.154253	626.035594	9.530407
7.682822	630.132949	9.535424
7.569181	610.740536	9.540442
7.663069	618.936317	9.545459
8.006289	629.312125	9.550477
7.740253	628.529924	9.555495
7.539290	626.054383	9.560512
8.001433	639.849450	9.565530
7.876755	646.742353	9.570547
7.961654	638.275964	9.575565
7.770592	637.055392	9.580583
7.381994	640.920347	9.585600
7.610280	638.966205	9.590618
7.517000	646.100349	9.595635
7.890744	646.566448	9.600653
7.626164	647.403191	9.605671
7.438528	644.179819	9.610688
7.594991	644.584857	9.615706
7.470693	652.496924	9.620723
7.704275	638.375179	9.625741
7.644444	658.580101	9.630759
8.044968	671.704342	9.635776
8.067303	673.241953	9.640794
7.910247	686.160129	9.645811
7.858732	683.564562	9.650829
7.837684	675.926866	9.655847
8.061823	686.315148	9.660864
8.006246	680.629896	9.665882
7.886788	678.657353	9.670899
8.127342	683.936939	9.675917
8.088595	673.152767	9.680935
8.254203	670.220874	9.685952
7.929513	652.160912	9.690970
7.862496	648.828989	9.695987
7.749809	659.229330	9.701005
8.201384	672.461252	9.706023
8.012511	676.211258	9.711040
8.198831	674.410508	9.716058
7.940502	673.106589	9.721075
8.067276	667.176594	9.726093
8.095841	668.518304	9.731111
7.956531	676.543689	9.736128
8.332023	671.493708	9.741146
8.150615	658.514020	9.746163
7.618069	656.714600	9.751181
7.721143	659.597808	9.756199
7.714750	673.743701	9.761216
8.083947	673.449973	9.766234
7.760928	686.329887	9.771251
7.837473	684.463461	9.776269
8.054190	686.971185	9.781287
8.195153	684.722855	9.786304
8.253371	681.938655	9.791322
8.026144	682.280269	9.796339
7.919879	674.661803	9.801357
8.213808	671.428757	9.806375
8.209066	678.609865	9.811392
8.229728	675.670872	9.816410
8.229389	672.993608	9.821427
8.238353	683.314769	9.826445
8.532681	674.695382	9.831463
8.041080	678.751014	9.836480
8.184168	678.065620	9.841498
8.389190	679.804462	9.846515
8.258237	678.355443	9.851533
8.287895	677.084933	9.856551
8.044100	686.911765	9.861568
8.219812	677.595921	9.866586
8.190242	681.914394	9.871603
8.245079	675.644361	9.876621
8.276205	677.251379	9.881639
8.276013	682.001967	9.886656
8.434907	668.842306	9.891674
8.146342	675.419271	9.896691
8.223997	677.608704	9.901709
8.303739	672.493924	9.906727
8.042271	673.077807	9.911744
8.161214	678.055895	9.916762
8.175582	677.320561	9.921779
8.121166	676.571421	9.926797
8.412946	671.174695	9.931815
8.171542	675.464075	9.936832
8.312960	690.059493	9.941850
8.351115	702.371771	9.946867
7.837202	706.127974	9.951885
8.559162	710.682617	9.956903
8.504218	702.443865	9.961920
8.688652	700.315492	9.966938
8.631505	707.209246	9.971955
8.456169	693.634465	9.976973
8.663246	687.160883	9.981991
8.110826	678.495104	9.987008
8.469845	684.380231	9.992026
8.488103	684.765048	9.997043
8.501025	683.352042	10.002061
8.606033	671.829939	10.007079
8.314847	683.334195	10.012096
8.457493	674.711973	10.017114
8.495468	686.021970	10.022131
8.224858	685.794032	10.027149
8.364411	685.683203	10.032167
7.883874	708.038629	10.037184
8.224794	709.469950	10.042202
8.319187	710.207099	10.047219
8.336944	712.624946	10.052237
8.423124	718.155683	10.057255
8.336689	723.524073	10.062272
8.512143	708.225150	10.067290
8.477300	716.707244	10.072307
8.326154	717.164993	10.077325
8.905602	704.636799	10.082343
8.692695	713.244434	10.087360
8.777796	712.440696	10.092378
8.780570	709.829048	10.097395
8.399051	714.120775	10.102413
8.685254	709.524517	10.107431
8.241949	719.136389	10.112448
8.327093	710.299274	10.117466
8.301042	707.690825	10.122483
8.169379	711.141621	10.127501
8.742692	726.397794	10.132519
8.815974	733.301456	10.137536
9.068441	724.357497	10.142554
8.771476	718.477572	10.147571
8.608467	709.176461	10.152589
9.040757	704.136355	10.157607
8.634240	711.559194	10.162624
8.756542	706.348778	10.167642
8.832401	699.785508	10.172659
8.392033	714.190296	10.177677
8.303356	708.293600	10.182695
8.552019	711.169244	10.187712
8.585365	709.411536	10.192730
8.653781	714.763335	10.197747
8.861661	731.298849	10.202765
9.251059	721.757842	10.207783
8.820239	716.275650	10.212800
9.018748	704.934090	10.217818
8.756341	709.808024	10.222835
8.465442	699.837588	10.227853
8.758388	701.918938	10.232871
8.759438	700.006747	10.237888
8.512720	706.929136	10.242906
8.448672	717.584044	10.247923
8.651112	727.699979	10.252941
8.620293	735.822383	10.257959
8.900942	744.105015	10.262976
9.068559	740.999557	10.267994
9.162076	739.558241	10.273011
9.126495	746.289790	10.278029
9.068827	726.558455	10.283047
8.876213	710.156770	10.288064
8.688265	705.172127	10.293082
8.800912	714.590368	10.298099
8.589237	731.529587	10.303117
9.079821	736.980375	10.308135
8.952476	746.320272	10.313152
8.838369	748.989868	10.318170
9.048251	742.092201	10.323187
8.970954	753.058364	10.328205
9.219759	737.870094	10.333223
9.030757	739.900160	10.338240
8.804392	737.659502	10.343258
8.871467	731.336242	10.348275
9.007520	746.729798	10.353293
9.172595	743.969622	10.358311
8.768334	742.554831	10.363328
9.045701	743.697484	10.368346
9.022645	734.321218	10.373363
8.675257	735.986590	10.378381
8.818038	736.086631	10.383399
8.743265	730.797429	10.388416
8.869631	741.104306	10.393434
9.055460	733.356739	10.398451
8.855925	738.915112	10.403469
8.827624	733.021399	10.408487
9.157646	736.304810	10.413504
8.945071	733.889832	10.418522
8.989704	734.475389	10.423539
9.056364	736.431626	10.428557
9.280345	744.510662	10.433575
9.318253	741.896733	10.438592
9.120592	750.991599	10.443610
9.227112	737.498446	10.448627
8.890666	748.087070	10.453645
9.098563	740.690156	10.458663
9.323183	735.369092	10.463680
9.101637	740.170918	10.468698
9.096776	745.938775	10.473715
8.630470	752.466863	10.478733
9.120156	741.747100	10.483751
9.192354	740.730549	10.488768
9.028997	749.169772	10.493786
9.594282	757.467873	10.498803
9.317981	754.702441	10.503821
9.264100	731.146681	10.508839
9.261521	741.427275	10.513856
8.942654	734.942344	10.518874
9.069437	744.618483	10.523891
9.239938	761.369655	10.528909
9.727906	765.048547	10.533927
9.427162	758.198422	10.538944
9.385542	739.016745	10.543962
9.380878	745.123525	10.548979
9.170038	754.423319	10.553997
9.149801	745.555212	10.559015
9.163226	739.556562	10.564032
9.217697	751.692172	10.569050
9.468786	754.400897	10.574067
9.055328	761.181640	10.579085
9.481502	761.266248	10.584103
9.749049	772.826072	10.589120
9.204375	766.443476	10.594138
9.717803	740.791120	10.599155
9.563566	751.987333	10.604173
9.621588	746.630470	10.609191
9.073824	740.148403	10.614208
9.213152	755.043029	10.619226
9.445658	739.049630	10.624243
9.484763	740.360862	10.629261
9.266372	744.843289	10.634279
9.024720	738.988840	10.639296
9.203475	758.534146	10.644314
9.383246	763.151422	10.649331
9.386493	769.067543	10.654349
9.904787	765.368609	10.659367
9.666886	772.317125	10.664384
9.369015	773.865253	10.669402
9.610484	765.647459	10.674419
9.331102	772.013508	10.679437
9.499031	767.798214	10.684455
9.524294	770.000273	10.689472
9.348460	786.824569	10.694490
9.766353	767.262059	10.699507
9.637139	774.332334	10.704525
9.923238	765.114687	10.709543
9.797425	777.232930	10.714560
9.521359	770.605471	10.719578
9.735833	772.050650	10.724595
9.584433	771.297487	10.729613
9.705883	763.871966	10.734631
9.783347	758.066236	10.739648
9.339809	758.145262	10.744666
9.813951	757.273164	10.749683
9.558744	770.679683	10.754701
9.370721	775.689343	10.759719
9.684513	766.587969	10.764736
9.727065	774.153000	10.769754
9.537251	772.949925	10.774771
9.497297	773.238878	10.779789
9.515476	779.160403	10.784807
9.585356	777.832046	10.789824
9.147278	769.321288	10.794842
9.440521	765.535613	10.799859
9.402245	773.162843	10.804877
9.408488	772.307597	10.809895
9.824964	776.567589	10.814912
9.611946	778.009152	10.819930
9.709466	786.759901	10.824947
9.978460	790.709298	10.829965
9.671833	790.859742	10.834983
9.642972	787.408485	10.840000
9.815844	803.755789	10.845018
10.217247	796.111070	10.850035
9.775967	784.797840	10.855053
9.880475	776.586185	10.860071
9.738268	771.466789	10.865088
9.481091	784.032355	10.870106
10.110268	787.967776	10.875123
9.578236	793.030075	10.880141
9.680252	801.023831	10.885159
10.085684	796.838095	10.890176
9.786664	807.137507	10.895194
10.132971	803.600108	10.900211
10.181399	805.448749	10.905229
9.996162	796.673679	10.910247
9.920374	775.070191	10.915264
10.004990	781.379118	10.920282
9.685958	774.824123	10.925299
10.072385	789.231434	10.930317
10.029284	789.187856	10.935335
9.920601	781.405574	10.940352
9.949616	798.961667	10.945370
9.761146	800.822765	10.950387
9.936073	807.043130	10.955405
10.043984	795.588167	10.960423
10.208449	798.535641	10.965440
10.310316	807.074669	10.970458
9.942068	790.616553	10.975475
9.971568	793.731642	10.980493
10.032971	794.408514	10.985511
10.202552	800.441977	10.990528
9.769925	803.432815	10.995546
9.964316	800.244964	11.000563
10.325423	811.259432	11.005581
10.228523	808.257996	11.010599
10.508057	802.932933	11.015616
10.315383	789.805796	11.020634
10.095413	779.466103	11.025651
10.065652	776.741728	11.030669
9.890422	776.073215	11.035687
10.240309	778.269156	11.040704
10.109554	792.455434	11.045722
10.078536	789.084451	11.050739
10.245484	800.701896	11.055757
9.964706	813.962302	11.060775
10.275887	799.256923	11.065792
10.004622	809.261205	11.070810
10.218084	809.691650	11.075827
10.152993	805.350768	11.080845
10.245606	796.673775	11.085863
10.319596	797.087159	11.090880
10.316869	806.954459	11.095898
10.245341	805.672349	11.100915
10.203291	803.398011	11.105933
9.997087	808.859486	11.110951
10.008364	810.576885	11.115968
10.252898	805.368242	11.120986
10.122263	804.071512	11.126003
10.097816	797.119715	11.131021
10.075883	809.310933	11.136039
10.348127	802.280479	11.141056
10.106952	800.481216	11.146074
10.108355	801.540837	11.151091
10.259843	804.706196	11.156109
10.256305	812.931992	11.161127
10.359946	811.770867	11.166144
10.382421	823.935847	11.171162
10.388827	831.439572	11.176179
11.061108	831.272416	11.181197
10.296097	819.566727	11.186215
10.676716	808.031166	11.191232
10.144718	808.258298	11.196250
10.446465	793.821795	11.201267
10.703070	796.462688	11.206285
10.691189	800.434583	11.211303
10.552176	796.849998	11.216320
10.631668	796.259377	11.221338
10.515075	808.113139	11.226355
10.557760	795.393063	11.231373
10.807404	799.017732	11.236391
10.568542	795.945322	11.241408
10.372814	804.339938	11.246426
10.628840	799.251041	11.251443
10.872778	805.145822	11.256461
10.266094	801.865829	11.261479
10.426116	801.345727	11.266496
10.214210	804.288206	11.271514
10.205147	809.092662	11.276531
10.485134	801.168455	11.281549
10.590965	811.670895	11.286567
10.598630	809.618232	11.291584
10.635294	814.628099	11.296602
10.362169	821.073835	11.301619
10.689960	826.466577	11.306637
10.593125	834.840503	11.311655
10.866413	832.604884	11.316672
10.642692	825.717566	11.321690
10.586570	832.970242	11.326707
10.752482	836.594219	11.331725
10.656599	826.313471	11.336743
10.996748	819.676860	11.341760
10.509763	843.184273	11.346778
10.681181	831.773096	11.351795
10.558465	828.039749	11.356813
10.430075	831.947485	11.361831
10.996401	831.343961	11.366848
10.675488	835.923308	11.371866
10.780560	824.306597	11.376883
10.706350	834.421171	11.381901
10.695617	831.554667	11.386919
10.855038	824.932234	11.391936
10.732922	832.403701	11.396954
10.915856	839.563254	11.401971
10.723403	832.476278	11.406989
10.608274	833.823294	11.412007
10.691619	832.493884	11.417024
10.864237	822.770219	11.422042
10.954963	828.110096	11.427059
10.880203	824.075124	11.432077
10.908578	829.212739	11.437095
10.980386	832.931821	11.442112
10.641008	830.106352	11.447130
10.966470	842.217631	11.452147
10.672884	833.762041	11.457165
10.398885	842.170425	11.462183
10.951917	851.507952	11.467200
10.767925	855.826061	11.472218
11.359677	856.227330	11.477235
11.205310	863.472274	11.482253
11.029586	857.495845	11.487271
10.996525	853.394515	11.492288
10.885897	847.922638	11.497306
11.021909	857.962261	11.502323
11.211368	856.191677	11.507341
11.130680	870.063453	11.512359
11.216170	850.185033	11.517376
11.174579	841.158999	11.522394
10.606817	832.456305	11.527411
11.338879	840.209932	11.532429
10.903554	855.891114	11.537447
11.094173	857.463079	11.542464
11.077536	865.136376	11.547482
11.198764	864.742768	11.552499
11.312458	859.827018	11.557517
11.319849	869.344668	11.562535
11.420988	841.375106	11.567552
11.230547	834.744070	11.572570
11.061865	826.703998	11.577587
11.135368	829.768503	11.582605
10.904985	834.247823	11.587623
11.139561	845.722222	11.592640
11.570593	856.304693	11.597658
11.278799	860.114697	11.602675
11.515578	846.895140	11.607693
10.907324	843.120936	11.612711
11.218147	848.404690	11.617728
11.353790	855.178402	11.622746
11.236202	861.207869	11.627763
11.439186	861.259361	11.632781
11.130968	871.466249	11.637799
11.453350	860.193823	11.642816
11.515180	872.338545	11.647834
10.893961	858.563845	11.652851
11.257694	861.457862	11.657869
11.223164	864.047375	11.662887
11.256942	859.085413	11.667904
11.358136	863.545267	11.672922
10.975431	866.120391	11.677939
11.502734	858.342201	11.682957
11.120059	861.188958	11.687975
11.421289	865.388536	11.692992
11.394376	861.536173	11.698010
11.235941	864.109197	11.703027
11.346497	860.441147	11.708045
11.602557	872.834401	11.713063
11.278572	866.129014	11.718080
11.350720	862.958636	11.723098
11.174276	866.040916	11.728115
11.621104	873.728412	11.733133
11.277691	888.808217	11.738151
11.341842	891.379819	11.743168
11.820985	894.095685	11.748186
11.562706	894.619601	11.753203
11.927503	881.880760	11.758221
11.566734	878.947805	11.763239
11.756575	866.400144	11.768256
11.915777	861.067036	11.773274
11.419629	862.435417	11.778291
11.560488	858.754869	11.783309
11.397962	872.626025	11.788327
11.353504	872.404728	11.793344
11.640749	868.787335	11.798362
11.616892	889.950529	11.803379
11.772347	893.481373	11.808397
11.496815	899.747235	11.813415
11.588752	896.238945	11.818432
11.678975	888.951598	11.823450
11.456159	895.035903	11.828467
11.429686	899.122439	11.833485
11.297015	898.677965	11.838503
11.658260	894.825488	11.843520
11.606301	887.163281	11.848538
11.681015	890.305940	11.853555
11.807366	897.133569	11.858573
11.784424	893.638396	11.863591
11.745178	891.897807	11.868608
11.968901	886.983512	11.873626
11.790781	893.560784	11.878643
12.100006	887.562306	11.883661
11.836537	901.687593	11.888679
11.433296	891.385259	11.893696
11.932962	886.594554	11.898714
11.744569	890.886238	11.903731
11.893095	888.659854	11.908749
12.015652	886.572803	11.913767
12.143795	888.771621	11.918784
11.833846	901.600339	11.923802
11.478187	899.533028	11.928819
11.720162	894.379106	11.933837
12.068103	897.934769	11.938855
11.978333	908.353527	11.943872
12.233960	896.222487	11.948890
12.073665	907.667440	11.953907
12.273343	896.154690	11.958925
11.979169	892.093044	11.963943
11.857331	895.954437	11.968960
12.417456	899.971003	11.973978
11.833682	893.209415	11.978995
12.073632	897.180971	11.984013
11.815818	897.956766	11.989031
11.775170	895.151500	11.994048
12.156299	894.323929	11.999066
11.845063	908.463825	12.004083
11.873141	919.152826	12.009101
12.007557	924.598488	12.014119
12.166951	930.130563	12.019136
12.483795	917.051224	12.024154
12.099343	924.181154	12.029171
12.309327	922.554008	12.034189
12.475702	929.941926	12.039207
12.334106	912.099362	12.044224
12.488282	900.037871	12.049242
11.760611	888.485781	12.054259
12.184987	890.029672	12.059277
12.412704	902.654797	12.064295
11.951226	905.042194	12.069312
12.345545	905.906451	12.074330
12.363877	926.261959	12.079347
12.831787	915.400021	12.084365
12.396506	897.537998	12.089383
11.951817	893.293805	12.094400
12.419838	884.812461	12.099418
12.341965	890.911344	12.104435
12.087727	884.994359	12.109453
12.106827	892.390505	12.114471
12.148541	912.383086	12.119488
12.212091	921.602112	12.124506
12.503130	921.802009	12.129523
12.582416	920.249259	12.134541
12.441090	927.178702	12.139559
12.469642	927.586623	12.144576
12.829536	924.828012	12.149594
12.584621	912.751891	12.154611
12.353652	897.717317	12.159629
12.207083	888.045678	12.164647
12.268238	906.313464	12.169664
12.570500	906.083963	12.174682
12.718914	921.242192	12.179699
12.585364	916.709475	12.184717
12.414153	893.053612	12.189735
12.082729	895.384828	12.194752
12.085882	904.631167	12.199770
12.125401	913.285298	12.204787
11.982945	920.971582	12.209805
11.985412	920.100025	12.214823
11.966774	925.065543	12.219840
12.683299	930.869914	12.224858
12.821289	942.376124	12.229875
12.800817	944.701918	12.234893
13.132816	934.802192	12.239911
12.668064	932.265168	12.244928
12.659487	920.393990	12.249946
12.633555	926.848835	12.254963
12.321562	927.470619	12.259981
12.658658	926.740491	12.264999
12.683370	934.560511	12.270016
12.935880	928.428108	12.275034
12.809701	933.446868	12.280051
12.455493	921.208532	12.285069
12.885331	928.186304	12.290087
12.719857	936.320481	12.295104
13.006860	938.811885	12.300122
12.560562	926.483680	12.305139
12.492703	932.711623	12.310157
12.492769	937.072108	12.315175
12.747374	941.472332	12.320192
13.067001	942.347778	12.325210
12.986313	940.599085	12.330227
12.608970	938.231042	12.335245
12.891026	942.160206	12.340263
12.853700	948.664977	12.345280
13.108144	947.572961	12.350298
13.209604	949.719517	12.355315
12.803743	951.669777	12.360333
13.223725	950.950725	12.365351
12.892782	955.738845	12.370368
13.207283	956.411606	12.375386
13.171477	955.832986	12.380403
12.602817	940.192506	12.385421
13.144324	945.008981	12.390439
12.535884	951.070552	12.395456
12.851071	950.065717	12.400474
12.865241	949.313081	12.405491
12.874271	955.709789	12.410509
13.300785	944.456672	12.415527
13.095188	945.166739	12.420544
13.290045	958.172531	12.425562
12.949468	948.231419	12.430579
12.840943	955.508184	12.435597
13.343502	956.860403	12.440615
13.105697	955.686913	12.445632
13.296787	948.580859	12.450650
13.230564	950.098124	12.455667
12.977849	947.289383	12.460685
13.258448	946.733170	12.465703
13.079571	952.860612	12.470720
12.981863	948.529815	12.475738
13.282233	939.055777	12.480755
12.871745	950.886270	12.485773
13.248537	941.652714	12.490791
12.962278	951.097785	12.495808
13.044554	950.433866	12.500826
13.059425	957.543355	12.505843
13.013612	951.725290	12.510861
13.107293	946.214036	12.515879
12.936642	959.322477	12.520896
13.424513	969.222022	12.525914
13.479380	976.617010	12.530931
13.331492	976.594719	12.535949
13.538695	970.256426	12.540967
13.172679	961.245067	12.545984
13.406804	973.406612	12.551002
13.101542	979.767188	12.556019
12.890218	983.418235	12.561037
13.353780	982.333713	12.566055
13.721457	980.218265	12.571072
13.802060	973.801331	12.576090
13.846575	975.523874	12.581107
13.746091	967.748014	12.586125
13.906645	949.850650	12.591143
13.535154	943.394029	12.596160
13.391573	948.321192	12.601178
13.389821	947.146802	12.606195
13.581800	945.388783	12.611213
13.472364	943.206681	12.616231
13.326556	948.639308	12.621248
13.532794	956.514709	12.626266
13.345513	957.205603	12.631283
13.218558	973.919650	12.636301
13.827541	977.231720	12.641319
13.856750	984.932522	12.646336
13.954430	977.506504	12.651354
13.637595	948.803633	12.656371
13.454610	951.591751	12.661389
13.428186	960.705232	12.666407
13.762834	974.525254	12.671424
13.524116	981.109841	12.676442
13.683428	978.481282	12.681459
13.519258	982.407578	12.686477
13.571435	975.070195	12.691495
13.640154	988.573650	12.696512
13.579116	981.916006	12.701530
13.627488	986.719273	12.706547
13.420199	993.817930	12.711565
13.596854	981.488886	12.716583
13.956977	985.399622	12.721600
13.636488	974.665831	12.726618
13.290976	980.807098	12.731635
13.515946	993.452044	12.736653
13.736804	986.189868	12.741671
13.641978	1011.599836	12.746688
13.882821	1003.383596	12.751706
13.845171	1004.961487	12.756723
13.566911	1006.428833	12.761741
14.113764	1003.469179	12.766759
14.352909	1001.970262	12.771776
14.072064	996.833591	12.776794
14.074968	1003.269127	12.781811
13.915024	995.691280	12.786829
14.324841	997.627340	12.791847
14.439509	1003.669188	12.796864
14.049289	993.712252	12.801882
14.085299	984.094569	12.806899
13.944974	972.293590	12.811917
14.393693	971.389078	12.816935
13.976582	977.948875	12.821952
14.053835	975.653182	12.826970
13.959605	968.601844	12.831987
13.789821	973.382967	12.837005
14.210653	980.622479	12.842023
13.922881	989.489503	12.847040
14.268993	1003.473393	12.852058
14.251388	988.704961	12.857075
14.230688	1000.302056	12.862093
14.369728	991.093668	12.867111
14.375887	976.339028	12.872128
13.810374	976.645329	12.877146
14.368718	979.226448	12.882163
14.120164	978.080719	12.887181
14.083155	978.367219	12.892199
13.839129	996.181731	12.897216
13.740265	995.832438	12.902234
14.389431	987.992668	12.907251
13.886778	1001.437604	12.912269
14.211923	991.724009	12.917287
13.879610	995.397455	12.922304
13.798411	999.841883	12.927322
14.021383	1006.271687	12.932339
14.517235	1028.627304	12.937357
14.488979	1022.027598	12.942375
14.602801	1032.539887	12.947392
14.363856	1022.572843	12.952410
14.358384	1021.934869	12.957427
14.276537	1025.767232	12.962445
14.257354	1034.747280	12.967463
14.617323	1033.474012	12.972480
14.624050	1033.479660	12.977498
14.642679	1025.652159	12.982515
14.454835	1042.813352	12.987533
14.449683	1033.403627	12.992551
14.691692	1036.811516	12.997568
14.705496	1028.642700	13.002586
14.603291	1027.300299	13.007603
14.651867	1038.170627	13.012621
14.909720	1012.153074	13.017639
14.730585	1003.687493	13.022656
14.508012	1000.151735	13.027674
14.967866	992.260637	13.032691
14.379643	994.776509	13.037709
15.032301	995.357847	13.042727
14.811458	998.444355	13.047744
14.353928	998.028475	13.052762
14.851606	990.204733	13.057779
14.486124	996.637097	13.062797
14.376566	992.407458	13.067815
14.580651	1006.416837	13.072832
14.462237	1021.981538	13.077850
14.940340	1025.011367	13.082867
14.712953	1032.595633	13.087885
14.818372	1022.688098	13.092903
14.853783	1021.309919	13.097920
14.689470	1028.320769	13.102938
14.898726	1022.380917	13.107955
14.896548	1033.648213	13.112973
14.692954	1027.814122	13.117991
14.768255	1028.156826	13.123008
14.577505	1025.494890	13.128026
14.996612	1017.181410	13.133043
14.705844	1035.686356	13.138061
14.689628	1027.101269	13.143079
14.978926	1036.637692	13.148096
14.829338	1031.537935	13.153114
14.993024	1025.472562	13.158131
14.662838	1028.471675	13.163149
15.169209	1028.518205	13.168167
14.766472	1024.453241	13.173184
14.636594	1027.105418	13.178202
15.552432	1014.004368	13.183219
14.681047	1028.281613	13.188237
14.952933	1027.860692	13.193255
14.949125	1027.570458	13.198272
15.054679	1048.060890	13.203290
15.339542	1046.149690	13.208307
15.151606	1043.049114	13.213325
15.101476	1029.106862	13.218343
15.264916	1030.108566	13.223360
15.152238	1031.881554	13.228378
15.336031	1026.590379	13.233395
14.933828	1022.991844	13.238413
15.460975	1026.624156	13.243431
15.548075	1033.635897	13.248448
15.127082	1027.266174	13.253466
15.197935	1016.815963	13.258483
15.084253	1023.935746	13.263501
15.266422	1025.568574	13.268519
15.307074	1031.550252	13.273536
15.359644	1046.889035	13.278554
15.515534	1030.960776	13.283571
15.277955	1033.902037	13.288589
14.978390	1038.001549	13.293607
15.139599	1047.802093	13.298624
15.257637	1055.115007	13.303642
15.463447	1051.211856	13.308659
15.501595	1055.250333	13.313677
15.640421	1058.798929	13.318695
15.794050	1058.728679	13.323712
15.362199	1056.695615	13.328730
15.719939	1059.122965	13.333747
15.630372	1043.411315	13.338765
15.644749	1035.969537	13.343783
15.372599	1022.755760	13.348800
15.396275	1027.683597	13.353818
15.809433	1043.050066	13.358835
15.598549	1033.596064	13.363853
15.689734	1031.550408	13.368871
15.355251	1027.987900	13.373888
15.198846	1036.721784	13.378906
15.604594	1040.682852	13.383923
15.713323	1059.550791	13.388941
15.725972	1051.540416	13.393959
15.615994	1059.422957	13.398976
15.351442	1054.778826	13.403994
15.696927	1051.229697	13.409011
15.673650	1059.717150	13.414029
15.436318	1051.128901	13.419047
15.642697	1046.681978	13.424064
15.543711	1051.297076	13.429082
15.824197	1053.469118	13.434099
15.696634	1060.899078	13.439117
15.776424	1056.034942	13.444135
16.042083	1050.707762	13.449152
15.821741	1058.772352	13.454170
15.987927	1047.644155	13.459187
15.574216	1054.785288	13.464205
15.664006	1051.027328	13.469223
16.055740	1054.545461	13.474240
15.604885	1052.298230	13.479258
15.952287	1045.526077	13.484275
16.203776	1051.468126	13.489293
15.550877	1053.790395	13.494311
15.486312	1052.475223	13.499328
15.492766	1065.006810	13.504346
15.915889	1078.344969	13.509363
15.965337	1083.433511	13.514381
16.196034	1079.118767	13.519399
16.143414	1084.888360	13.524416
15.937294	1085.429234	13.529434
16.099669	1090.914812	13.534451
16.154872	1085.051231	13.539469
16.300451	1083.788657	13.544487
16.409257	1089.790173	13.549504
16.026437	1081.683068	13.554522
16.235964	1061.309448	13.559539
16.139820	1056.200045	13.564557
15.951314	1059.699699	13.569575
16.431067	1067.886939	13.574592
16.137061	1065.153909	13.579610
16.007816	1078.001666	13.584627
16.056088	1075.945394	13.589645
16.157128	1089.568777	13.594663
16.266700	1074.963842	13.599680
16.274918	1084.186616	13.604698
16.373281	1084.334172	13.609715
16.389654	1090.763183	13.614733
16.358325	1087.224869	13.619751
16.477737	1088.632278	13.624768
16.587861	1084.348128	13.629786
16.487436	1096.244706	13.634803
16.343753	1094.946569	13.639821
16.103763	1090.064510	13.644839
16.294523	1088.244081	13.649856
16.062643	1089.881701	13.654874
16.355844	1089.047028	13.659891
16.412447	1078.512917	13.664909
16.262626	1089.383457	13.669927
16.602541	1083.436906	13.674944
16.334398	1079.451211	13.679962
16.281835	1088.321861	13.684979
16.283166	1078.332317	13.689997
16.316633	1087.870979	13.695015
16.737214	1082.430737	13.700032
16.337260	1086.894115	13.705050
16.594285	1094.012386	13.710067
16.550162	1086.907424	13.715085
16.054600	1093.742061	13.720103
16.671440	1099.511430	13.725120
16.794392	1111.493468	13.730138
16.498523	1108.395397	13.735155
16.829372	1108.535556	13.740173
16.686698	1113.996067	13.745191
16.795388	1109.334995	13.750208
16.766551	1108.715058	13.755226
16.983600	1107.867799	13.760243
16.926423	1108.428104	13.765261
16.808236	1111.533461	13.770279
16.999956	1100.610046	13.775296
16.679368	1109.142819	13.780314
16.771699	1103.128207	13.785331
17.218434	1103.009816	13.790349
16.813724	1106.390561	13.795367
17.065146	1098.409519	13.800384
16.675953	1098.681113	13.805402
17.025325	1098.171378	13.810419
17.064604	1098.903894	13.815437
16.917465	1103.160065	13.820455
16.986900	1098.365344	13.825472
16.833662	1098.475037	13.830490
17.003132	1100.542638	13.835507
16.981960	1099.785217	13.840525
17.270870	1101.627929	13.845543
17.302719	1094.810372	13.850560
16.744202	1079.399953	13.855578
16.798931	1087.961902	13.860595
17.070921	1096.634725	13.865613
16.982628	1101.304759	13.870631
16.999367	1101.122535	13.875648
16.852930	1105.909675	13.880666
17.015035	1099.373292	13.885683
16.986198	1104.490945	13.890701
16.881913	1101.834363	13.895719
16.986195	1101.620321	13.900736
17.186003	1103.307715	13.905754
17.197293	1098.949379	13.910771
17.433953	1098.671686	13.915789
17.306009	1099.983446	13.920807
17.610945	1096.991002	13.925824
17.477045	1092.982681	13.930842
17.166132	1097.375809	13.935859
17.595384	1096.333574	13.940877
17.096374	1101.692855	13.945895
17.232766	1102.557709	13.950912
16.925509	1100.454403	13.955930
16.942857	1096.799763	13.960947
17.220130	1102.566702	13.965965
17.218586	1121.799028	13.970983
17.474412	1127.547481	13.976000
17.626955	1128.806105	13.981018
17.504087	1139.321835	13.986035
17.916911	1125.237092	13.991053
17.334029	1129.209531	13.996071
17.592767	1123.851190	14.001088
17.811551	1126.433446	14.006106
17.632304	1122.596006	14.011123
17.840559	1111.803699	14.016141
17.292726	1108.255241	14.021159
17.801543	1115.127111	14.026176
17.766856	1121.776787	14.031194
17.450060	1107.666424	14.036211
17.643223	1110.497399	14.041229
17.800256	1117.064935	14.046247
17.477294	1117.079508	14.051264
17.789837	1124.557878	14.056282
17.708306	1122.488843	14.061299
17.872312	1122.317271	14.066317
17.546272	1123.170514	14.071335
17.550604	1123.935588	14.076352
17.756682	1121.542166	14.081370
17.864085	1121.701610	14.086387
18.140749	1114.367932	14.091405
17.608015	1128.744697	14.096423
17.779049	1122.068642	14.101440
17.887835	1124.912804	14.106458
17.908103	1125.760275	14.111475
18.007853	1120.301495	14.116493
17.979139	1120.450015	14.121511
17.998738	1119.123263	14.126528
17.838678	1124.785862	14.131546
17.898755	1118.869889	14.136563
18.043978	1112.729983	14.141581
18.139274	1124.857157	14.146599
18.056521	1113.801629	14.151616
18.313357	1122.485637	14.156634
17.963402	1122.913327	14.161651
18.114507	1113.598541	14.166669
18.100082	1122.701076	14.171687
17.937752	1118.732494	14.176704
17.993259	1113.365292	14.181722
17.790357	1116.997652	14.186739
18.290843	1115.774336	14.191757
18.045310	1119.922793	14.196775
18.205542	1115.906705	14.201792
18.365242	1118.754246	14.206810
17.769706	1110.337479	14.211827
18.458459	1112.034459	14.216845
18.393457	1119.349368	14.221863
18.235407	1115.908406	14.226880
18.234696	1112.839016	14.231898
17.760355	1114.928190	14.236915
18.350120	1117.737980	14.241933
18.276765	1130.376926	14.246951
18.787233	1137.620961	14.251968
18.806096	1119.556319	14.256986
18.581736	1122.227306	14.262003
18.588953	1110.014796	14.267021
18.259406	1111.077667	14.272039
18.513350	1107.248418	14.277056
18.622196	1102.352685	14.282074
18.320987	1108.934682	14.287091
18.647142	1105.991477	14.292109
18.724915	1114.386639	14.297127
18.506115	1114.689465	14.302144
18.544640	1104.450446	14.307162
18.450287	1115.114975	14.312179
18.679793	1108.466250	14.317197
18.611436	1118.633188	14.322215
18.799967	1114.137234	14.327232
18.733667	1106.523354	14.332250
18.555857	1109.431898	14.337267
18.699921	1114.931540	14.342285
18.720775	1113.296324	14.347303
18.397683	1110.955883	14.352320
18.458229	1127.280792	14.357338
18.536009	1135.027561	14.362355
18.940327	1129.690780	14.367373
18.720388	1139.689531	14.372391
18.617619	1144.297410	14.377408
18.880722	1134.241649	14.382426
18.757820	1147.677370	14.387443
18.686641	1137.892307	14.392461
18.789622	1141.883852	14.397479
18.843642	1141.320270	14.402496
18.985705	1142.838103	14.407514
18.664501	1143.053952	14.412531
18.944108	1138.595271	14.417549
18.952124	1147.487025	14.422567
18.639407	1138.988766	14.427584
18.884078	1136.458247	14.432602
18.796089	1142.580163	14.437619
18.817375	1150.491407	14.442637
19.117753	1166.841997	14.447655
19.208383	1163.726370	14.452672
19.462164	1168.753153	14.457690
19.147618	1168.123833	14.462707
19.272836	1166.475267	14.467725
19.282024	1146.175258	14.472743
18.739746	1143.767567	14.477760
19.156008	1154.125532	14.482778
18.945974	1157.721682	14.487795
19.419834	1166.561899	14.492813
19.357123	1162.116588	14.497831
19.537014	1162.425442	14.502848
19.593907	1159.422880	14.507866
19.412927	1155.338876	14.512883
19.380606	1148.838604	14.517901
19.122461	1144.043784	14.522919
19.184435	1153.423834	14.527936
19.189027	1159.533575	14.532954
18.887371	1175.397268	14.537971
19.183067	1168.239541	14.542989
19.380681	1171.341042	14.548007
19.174045	1176.165335	14.553024
19.483480	1166.679423	14.558042
19.377006	1168.930123	14.563059
19.271813	1164.458777	14.568077
19.486492	1170.714438	14.573095
19.406022	1173.412000	14.578112
19.511344	1166.206273	14.583130
19.647838	1169.468676	14.588147
20.125387	1167.303515	14.593165
19.757451	1169.784512	14.598183
19.601792	1167.182093	14.603200
19.967404	1167.260200	14.608218
19.513996	1178.109420	14.613235
19.490493	1173.232037	14.618253
19.727513	1165.082878	14.623271
19.991624	1169.441437	14.628288
19.830835	1168.235493	14.633306
19.518826	1170.776519	14.638323
19.376157	1163.155178	14.643341
19.317884	1175.576317	14.648359
19.607364	1190.270127	14.653376
20.073698	1190.750834	14.658394
19.574253	1198.033390	14.663411
19.993223	1197.278670	14.668429
20.168866	1203.388057	14.673447
20.108058	1200.840397	14.678464
20.039982	1197.192398	14.683482
19.827057	1196.878916	14.688499
20.068729	1201.445918	14.693517
20.123988	1196.455882	14.698535
19.839814	1195.711299	14.703552
20.432098	1192.803929	14.708570
20.093205	1199.096149	14.713587
20.118681	1201.615547	14.718605
20.126725	1191.657101	14.723623
19.663993	1192.724314	14.728640
20.271102	1195.405660	14.733658
20.245717	1203.262457	14.738675
20.103529	1191.724209	14.743693
19.934279	1189.631502	14.748711
19.964053	1195.520559	14.753728
20.022416	1190.289467	14.758746
20.059920	1200.087758	14.763763
19.844856	1191.540624	14.768781
19.860902	1190.177054	14.773799
19.898681	1203.702355	14.778816
20.658525	1206.720606	14.783834
20.653974	1224.451632	14.788851
20.599812	1217.891170	14.793869
20.232546	1195.129490	14.798887
20.166406	1216.918223	14.803904
20.753771	1219.871340	14.808922
20.919210	1219.127893	14.813939
20.905519	1202.889752	14.818957
20.636771	1188.333183	14.823975
20.202162	1194.606607	14.828992
20.200826	1187.064211	14.834010
20.415283	1183.137549	14.839027
20.093263	1195.742924	14.844045
20.614680	1204.256793	14.849063
20.841546	1216.595317	14.854080
20.984467	1210.121905	14.859098
20.808793	1203.415040	14.864115
20.733459	1194.825082	14.869133
20.854778	1185.058506	14.874151
20.811816	1189.582088	14.879168
20.931292	1189.622214	14.884186
20.545637	1175.912549	14.889203
20.529664	1183.853208	14.894221
20.845757	1175.121676	14.899239
20.816623	1182.920424	14.904256
20.793252	1176.567866	14.909274
20.608889	1174.100510	14.914291
20.595675	1186.468922	14.919309
21.302569	1203.731735	14.924327
21.022481	1197.431126	14.929344
20.815960	1184.863016	14.934362
21.093497	1193.109398	14.939379
21.044499	1189.563751	14.944397
21.256359	1179.053074	14.949415
20.771181	1176.509942	14.954432
20.910921	1170.393362	14.959450
20.956450	1172.814163	14.964467
20.786918	1195.692394	14.969485
21.195919	1201.757627	14.974503
20.780337	1212.670685	14.979520
21.099962	1214.846898	14.984538
21.006108	1214.869989	14.989555
21.198855	1214.830662	14.994573
21.487001	1210.828800	14.999591
21.203997	1213.727224	15.004608
21.642488	1217.510087	15.009626
21.261969	1218.968795	15.014643
21.574287	1214.366097	15.019661
21.853646	1196.902306	15.024679
21.411486	1195.483510	15.029696
21.450008	1185.568050	15.034714
21.098882	1178.196174	15.039731
20.993346	1180.937257	15.044749
21.248907	1182.952820	15.049767
21.142139	1199.035833	15.054784
21.294712	1200.890898	15.059802
21.203425	1208.501530	15.064819
21.367633	1214.085271	15.069837
21.697959	1202.281771	15.074855
21.470310	1222.362267	15.079872
21.688262	1206.766455	15.084890
21.328491	1214.724689	15.089907
21.472007	1216.274964	15.094925
21.951822	1208.452892	15.099943
21.431660	1211.094925	15.104960
21.536062	1216.760221	15.109978
21.713547	1208.605544	15.114995
21.702629	1207.611781	15.120013
21.628073	1206.128963	15.125031
21.377892	1217.313446	15.130048
21.447135	1210.901052	15.135066
21.387853	1206.996877	15.140083
21.265249	1214.239875	15.145101
21.749183	1219.621860	15.150119
21.708816	1241.251246	15.155136
21.792526	1235.871458	15.160154
21.660414	1225.959818	15.165171
21.705123	1235.042785	15.170189
22.059035	1235.320463	15.175207
21.934854	1234.432458	15.180224
21.731610	1230.605264	15.185242
22.118920	1244.993565	15.190259
21.852455	1240.045765	15.195277
22.066361	1238.550217	15.200295
21.833425	1242.413952	15.205312
22.002874	1238.464414	15.210330
22.240650	1235.869669	15.215347
21.898742	1238.437703	15.220365
22.314925	1226.612094	15.225383
22.192729	1228.453213	15.230400
22.414312	1226.804431	15.235418
22.100925	1229.193336	15.240435
21.846992	1234.586094	15.245453
22.328639	1227.176689	15.250471
22.290433	1232.462467	15.255488
22.199000	1230.409623	15.260506
22.454098	1224.203055	15.265523
22.316427	1230.365908	15.270541
22.475300	1228.733022	15.275559
22.428469	1234.654463	15.280576
22.145130	1226.902058	15.285594
22.493061	1230.503862	15.290611
22.221283	1239.982142	15.295629
22.492990	1227.418665	15.300647
22.346674	1230.102337	15.305664
22.140841	1226.053532	15.310682
22.560080	1223.942506	15.315699
22.555793	1224.379100	15.320717
22.654213	1228.908809	15.325735
22.805542	1231.055807	15.330752
22.626009	1224.774756	15.335770
22.768639	1219.381280	15.340787
22.069134	1229.480364	15.345805
22.295831	1229.645252	15.350823
22.405250	1241.417433	15.355840
22.625465	1250.448513	15.360858
22.652349	1248.922911	15.365875
22.927842	1261.226648	15.370893
22.778148	1256.913821	15.375911
22.766712	1264.675821	15.380928
22.869526	1253.303253	15.385946
22.957008	1259.741819	15.390963
23.153465	1260.777834	15.395981
23.184317	1250.371096	15.400999
23.035441	1255.657491	15.406016
23.027262	1237.123973	15.411034
22.987101	1229.114377	15.416051
22.922915	1225.307464	15.421069
22.816498	1222.368938	15.426087
22.794950	1236.206051	15.431104
23.237014	1250.839615	15.436122
23.588637	1249.808651	15.441139
22.801358	1245.932890	15.446157
23.496268	1230.362404	15.451175
22.869489	1226.538415	15.456192
23.103342	1223.194736	15.461210
23.502772	1224.323907	15.466227
23.201875	1230.420090	15.471245
23.158481	1220.613445	15.476263
23.108095	1219.169536	15.481280
23.394843	1222.390536	15.486298
23.313275	1214.636615	15.491315
23.126702	1228.583723	15.496333
23.459076	1235.359277	15.501351
23.303607	1234.058354	15.506368
22.969751	1246.418099	15.511386
23.038167	1246.359596	15.516403
23.288044	1247.746204	15.521421
23.536636	1250.124732	15.526439
23.557020	1258.447981	15.531456
23.152826	1249.866779	15.536474
23.357067	1248.990925	15.541491
23.306756	1262.416300	15.546509
23.345640	1250.040566	15.551527
23.211238	1257.306009	15.556544
23.576030	1255.766972	15.561562
23.634036	1246.616731	15.566579
23.454638	1255.429740	15.571597
23.712400	1250.609693	15.576615
23.458469	1244.518508	15.581632
23.198718	1242.784864	15.586650
23.889166	1263.305106	15.591667
23.934839	1280.490885	15.596685
24.154988	1269.540991	15.601703
23.983855	1259.136985	15.606720
23.830257	1249.261958	15.611738
23.847747	1247.624135	15.616755
23.759424	1240.221704	15.621773
23.846986	1245.583903	15.626791
23.750614	1245.594812	15.631808
23.561243	1251.348528	15.636826
24.070817	1261.245851	15.641843
23.904530	1271.234227	15.646861
24.125237	1269.958805	15.651879
24.250116	1267.872500	15.656896
24.108420	1269.929052	15.661914
24.650398	1269.625603	15.666931
23.901397	1260.982596	15.671949
23.721527	1247.559649	15.676967
24.118433	1258.253164	15.681984
24.273558	1267.402117	15.687002
24.497154	1257.287859	15.692019
23.986338	1262.015307	15.697037
23.947977	1266.578700	15.702055
24.253698	1274.848017	15.707072
24.082530	1276.291749	15.712090
24.352376	1283.129645	15.717107
24.044032	1273.409357	15.722125
24.214841	1276.009424	15.727143
24.458830	1271.656207	15.732160
24.085347	1275.196380	15.737178
24.172993	1273.098524	15.742195
24.302550	1270.620115	15.747213
24.537863	1268.255294	15.752231
24.218816	1265.186618	15.757248
24.420365	1268.392602	15.762266
24.590071	1268.520472	15.767283
24.540085	1274.439301	15.772301
24.616024	1279.560134	15.777319
24.385979	1283.500957	15.782336
24.915425	1287.203030	15.787354
24.872296	1281.456443	15.792371
24.726540	1277.550034	15.797389
24.529858	1278.759808	15.802407
24.570990	1272.222913	15.807424
24.693455	1293.879345	15.812442
24.766765	1304.576870	15.817459
24.627268	1307.446431	15.822477
24.649481	1310.765975	15.827495
25.144329	1304.088978	15.832512
25.031057	1305.158174	15.837530
25.304156	1292.723938	15.842547
25.208880	1294.579111	15.847565
24.932468	1276.323814	15.852583
24.899626	1269.656259	15.857600
25.014814	1271.415163	15.862618
25.113158	1267.774236	15.867635
25.125255	1265.700701	15.872653
25.008894	1259.335948	15.877671
25.236135	1255.175268	15.882688
24.697407	1256.603878	15.887706
25.128935	1264.255917	15.892723
24.877607	1274.303258	15.897741
24.903944	1282.531442	15.902759
25.088655	1287.978747	15.907776
24.982681	1298.711860	15.912794
24.984070	1294.374006	15.917811
24.958677	1299.371470	15.922829
25.153343	1301.531381	15.927847
25.257125	1291.562923	15.932864
25.065271	1297.251715	15.937882
25.363404	1287.372334	15.942899
25.079406	1293.679911	15.947917
25.108970	1301.165462	15.952935
24.872182	1300.657115	15.957952
25.223602	1310.140116	15.962970
25.221421	1306.108748	15.967987
25.587030	1310.352905	15.973005
25.109187	1312.297805	15.978023
25.559988	1309.558326	15.983040
25.505834	1314.140883	15.988058
25.673414	1309.203077	15.993075
25.483907	1311.972654	15.998093
25.314063	1310.452062	16.003111
25.491189	1309.539751	16.008128
25.403200	1338.928955	16.013146
25.518828	1344.804246	16.018163
25.846274	1338.649432	16.023181
25.943339	1342.048320	16.028199
26.113703	1326.197675	16.033216
26.036701	1341.490097	16.038234
26.306434	1336.069628	16.043251
26.111811	1324.591931	16.048269
26.234247	1316.008527	16.053287
26.186641	1304.932869	16.058304
25.985561	1294.631040	16.063322
26.000355	1303.135943	16.068339
26.056373	1304.329859	16.073357
26.020666	1298.176534	16.078375
25.746247	1301.445590	16.083392
25.876495	1312.267548	16.088410
26.031027	1317.854897	16.093427
26.424800	1333.305179	16.098445
26.379577	1343.801891	16.103463
26.329788	1307.022410	16.108480
26.261263	1301.180416	16.113498
26.367911	1294.840532	16.118515
26.537746	1304.977205	16.123533
26.134560	1304.420822	16.128551
26.380361	1296.051642	16.133568
26.261090	1305.572424	16.138586
26.315826	1299.782853	16.143603
26.414966	1303.543979	16.148621
26.296611	1303.386485	16.153639
26.809049	1298.756924	16.158656
26.351913	1314.908703	16.163674
26.659761	1302.426974	16.168691
26.537129	1297.274241	16.173709
26.367931	1294.137047	16.178727
26.592387	1300.893492	16.183744
26.495210	1322.843416	16.188762
26.782747	1317.864878	16.193779
26.790002	1323.446302	16.198797
26.682922	1323.739687	16.203815
26.597735	1322.741679	16.208832
26.731097	1321.832283	16.213850
26.593511	1327.859730	16.218867
26.673367	1318.758584	16.223885
26.575150	1327.301504	16.228903
26.684285	1326.439426	16.233920
26.529693	1330.817757	16.238938
26.627977	1333.325121	16.243955
26.737735	1323.230458	16.248973
26.537624	1331.543802	16.253991
26.584369	1327.022840	16.259008
26.630637	1332.789930	16.264026
26.658719	1348.896044	16.269043
27.212701	1346.035933	16.274061
26.991957	1358.832146	16.279079
27.730122	1359.040688	16.284096
27.389938	1364.399741	16.289114
26.839963	1339.502395	16.294131
27.444940	1345.771451	16.299149
27.396722	1354.429726	16.304167
27.261254	1346.409867	16.309184
27.044088	1340.394444	16.314202
27.154742	1347.114243	16.319219
27.209282	1354.692139	16.324237
26.988984	1360.437631	16.329255
27.905405	1343.365028	16.334272
27.458160	1364.610000	16.339290
27.351023	1358.932643	16.344307
27.488965	1352.359999	16.349325
27.414015	1353.063804	16.354343
27.436414	1349.090557	16.359360
27.397531	1356.037480	16.364378
27.738483	1351.421733	16.369395
27.690653	1354.392656	16.374413
27.414807	1352.167580	16.379431
27.478071	1353.861865	16.384448
27.442902	1354.863014	16.389466
27.497932	1357.235421	16.394483
27.620409	1351.461385	16.399501
27.662232	1355.673344	16.404519
27.796448	1352.196532	16.409536
27.845346	1352.066066	16.414554
27.681857	1348.564143	16.419571
27.708202	1347.537823	16.424589
27.364589	1349.803014	16.429607
27.911053	1341.441109	16.434624
27.445786	1359.707624	16.439642
27.626814	1366.914588	16.444659
27.997287	1372.722495	16.449677
28.107895	1387.800436	16.454695
28.382729	1380.714176	16.459712
28.283458	1384.794785	16.464730
28.075797	1377.128196	16.469747
28.421745	1379.610699	16.474765
28.019197	1385.732042	16.479783
28.315779	1379.166975	16.484800
28.737665	1363.506529	16.489818
28.135763	1358.941000	16.494835
28.063594	1349.055969	16.499853
28.014033	1352.735038	16.504871
28.143349	1364.333549	16.509888
28.230068	1369.383338	16.514906
28.309488	1377.520107	16.519923
28.590296	1375.728828	16.524941
28.388594	1380.073636	16.529959
28.377348	1371.607218	16.534976
28.423763	1370.455922	16.539994
28.486966	1370.967957	16.545011
28.396510	1375.400246	16.550029
28.444538	1379.137964	16.555047
28.604871	1373.708827	16.560064
28.757689	1374.883964	16.565082
28.417563	1371.862850	16.570099
28.442413	1368.636817	16.575117
28.290712	1382.342072	16.580135
28.333574	1373.185997	16.585152
28.558338	1371.191010	16.590170
28.567766	1369.654901	16.595187
28.421388	1378.162518	16.600205
28.576391	1390.691425	16.605223
28.646039	1393.551959	16.610240
28.837956	1401.157523	16.615258
28.779907	1389.961882	16.620275
28.669964	1396.504061	16.625293
28.820042	1399.598913	16.630311
28.913381	1400.994133	16.635328
29.075566	1408.062113	16.640346
28.566190	1417.281816	16.645363
29.218924	1399.020157	16.650381
29.165985	1399.210486	16.655399
29.338123	1402.036729	16.660416
29.237815	1399.717620	16.665434
28.841709	1405.320195	16.670451
29.180158	1398.444649	16.675469
28.965310	1401.666068	16.680487
29.230315	1409.155993	16.685504
29.450030	1413.857794	16.690522
29.553473	1431.823140	16.695539
29.545377	1403.281291	16.700557
29.203598	1396.386101	16.705575
29.334291	1414.825647	16.710592
29.328025	1420.491233	16.715610
29.620167	1426.076307	16.720627
29.913060	1421.917310	16.725645
29.563843	1406.525840	16.730663
29.594844	1401.632274	16.735680
29.375185	1395.245988	16.740698
29.410309	1421.086676	16.745715
29.603228	1420.480794	16.750733
29.480709	1427.267584	16.755751
29.662463	1415.844030	16.760768
29.855742	1416.924676	16.765786
29.544948	1425.248130	16.770803
30.031172	1416.356011	16.775821
29.832660	1420.646760	16.780839
29.784976	1421.162985	16.785856
29.969321	1416.333390	16.790874
29.200131	1415.610446	16.795891
29.703937	1422.797453	16.800909
29.777151	1424.080655	16.805927
29.698706	1423.703956	16.810944
30.133889	1420.736734	16.815962
29.854955	1423.504209	16.820979
30.034105	1433.559111	16.825997
30.373317	1440.196617	16.831015
30.385192	1444.198995	16.836032
30.164387	1418.187975	16.841050
30.141407	1416.659984	16.846067
30.335186	1410.927268	16.851085
30.558555	1423.163783	16.856103
30.554170	1416.096577	16.861120
30.376437	1411.857245	16.866138
30.259820	1415.438773	16.871155
30.383520	1405.263403	16.876173
30.529414	1415.656866	16.881191
30.309449	1408.137966	16.886208
30.807593	1410.518896	16.891226
30.174416	1413.159990	16.896243
30.583818	1412.594639	16.901261
30.427200	1413.343859	16.906279
30.518316	1405.036454	16.911296
30.723916	1406.897330	16.916314
30.643174	1407.769417	16.921331
30.528874	1408.158879	16.926349
30.515644	1417.042495	16.931367
30.595862	1438.320304	16.936384
30.943087	1436.005824	16.941402
30.785320	1447.738547	16.946419
30.856578	1443.378845	16.951437
30.796612	1442.419173	16.956455
30.668696	1449.093875	16.961472
30.808965	1443.462133	16.966490
30.522539	1447.378869	16.971507
30.615463	1442.070317	16.976525
30.486909	1442.379464	16.981543
30.941286	1447.951068	16.986560
30.796933	1449.563602	16.991578
30.790361	1452.184803	16.996595
31.208005	1461.769923	17.001613
31.171252	1474.095612	17.006631
31.138908	1477.191946	17.011648
31.335606	1474.052395	17.016666
31.408273	1482.859228	17.021683
31.530873	1460.005806	17.026701
31.517176	1449.832292	17.031719
30.924424	1440.314895	17.036736
31.586757	1450.561450	17.041754
31.549944	1470.311459	17.046771
31.346566	1452.323385	17.051789
31.746088	1454.937580	17.056807
31.189047	1446.144572	17.061824
31.779944	1447.628272	17.066842
31.556546	1446.265746	17.071859
31.511286	1436.731710	17.076877
31.429825	1449.849024	17.081895
31.249647	1461.745703	17.086912
31.623777	1457.243328	17.091930
31.459522	1456.171790	17.096947
31.890722	1463.391705	17.101965
31.846937	1457.679806	17.106983
31.505506	1465.552454	17.112000
31.890511	1463.701393	17.117018
31.650512	1459.437714	17.122035
31.842528	1467.216520	17.127053
31.936008	1467.125521	17.132071
31.794954	1465.969040	17.137088
31.983538	1458.227744	17.142106
32.003345	1467.745280	17.147123
31.905563	1462.233657	17.152141
31.808424	1466.269839	17.157159
31.686199	1467.189349	17.162176
31.964622	1475.714473	17.167194
31.753296	1483.157717	17.172211
31.917136	1485.171973	17.177229
32.189152	1484.596691	17.182247
32.091994	1498.862302	17.187264
32.375687	1484.420669	17.192282
32.174927	1495.938109	17.197299
32.323254	1482.244081	17.202317
32.687944	1490.773432	17.207335
32.387732	1491.980286	17.212352
32.545757	1481.764538	17.217370
32.285319	1489.019462	17.222387
32.682814	1488.013172	17.227405
32.825997	1484.983266	17.232423
32.451555	1486.441779	17.237440
32.776954	1476.076273	17.242458
32.751782	1481.695406	17.247475
32.661683	1484.945791	17.252493
32.591037	1483.270570	17.257511
32.585610	1483.201066	17.262528
32.702694	1479.227069	17.267546
32.440174	1483.578826	17.272563
32.813375	1481.763182	17.277581
32.862903	1476.217712	17.282599
32.706171	1469.165472	17.287616
32.948529	1482.603993	17.292634
32.907235	1483.000659	17.297651
33.181163	1495.151695	17.302669
33.132107	1486.587144	17.307687
33.234191	1485.574258	17.312704
33.160402	1476.546491	17.317722
33.100514	1481.524136	17.322739
33.301215	1481.249243	17.327757
33.300122	1474.294456	17.332775
33.050006	1475.791042	17.337792
33.277699	1470.644021	17.342810
33.308703	1478.817600	17.347827
33.044747	1476.417704	17.352845
32.997976	1489.895051	17.357863
33.516977	1507.869628	17.362880
33.431174	1497.278499	17.367898
33.728225	1509.782800	17.372915
33.670142	1510.431851	17.377933
33.857859	1502.413513	17.382951
33.336705	1490.244099	17.387968
33.496786	1475.639873	17.392986
33.428352	1488.146014	17.398003
33.305293	1504.355269	17.403021
34.100648	1507.220067	17.408039
33.712696	1505.552502	17.413056
34.045301	1508.502587	17.418074
33.892308	1515.230288	17.423091
33.661048	1508.558871	17.428109
33.739034	1507.077931	17.433127
33.722579	1504.909093	17.438144
34.020610	1504.133048	17.443162
33.560858	1501.585650	17.448179
33.661335	1510.659150	17.453197
33.543662	1504.679550	17.458215
33.917282	1503.189815	17.463232
34.012093	1500.444685	17.468250
33.761418	1498.961081	17.473267
33.753382	1514.322961	17.478285
34.066325	1522.197125	17.483303
33.707841	1521.470340	17.488320
34.036137	1531.267541	17.493338
34.045289	1523.774031	17.498355
34.018459	1528.716297	17.503373
34.254582	1528.012707	17.508391
34.036044	1541.278779	17.513408
34.230808	1535.336014	17.518426
34.365782	1540.600701	17.523443
34.678864	1555.279927	17.528461
34.621648	1544.412774	17.533479
34.372542	1543.420241	17.538496
34.715500	1547.263494	17.543514
34.874321	1553.060847	17.548531
34.542248	1534.630604	17.553549
34.795591	1523.778184	17.558567
34.256370	1536.746961	17.563584
34.637202	1544.097301	17.568602
34.764993	1555.465107	17.573619
34.905660	1564.219388	17.578637
35.033692	1560.875837	17.583655
35.086132	1561.437692	17.588672
35.084895	1558.208065	17.593690
35.155967	1530.859951	17.598707
34.673001	1522.991633	17.603725
35.065427	1527.122750	17.608743
34.890452	1554.402769	17.613760
35.012377	1551.704321	17.618778
34.940524	1561.420556	17.623795
35.184046	1563.218086	17.628813
35.583667	1553.579998	17.633831
35.178773	1560.041952	17.638848
35.226608	1551.323921	17.643866
35.474397	1558.451811	17.648883
35.232441	1557.463605	17.653901
35.241466	1554.944086	17.658919
35.041399	1554.569412	17.663936
35.355081	1553.357312	17.668954
35.247750	1551.471623	17.673971
35.200159	1549.613444	17.678989
35.650653	1550.249150	17.684007
35.501635	1558.602973	17.689024
35.622756	1552.978299	17.694042
35.711856	1542.629829	17.699059
35.607246	1550.968421	17.704077
35.912678	1545.679764	17.709095
35.747356	1550.362687	17.714112
35.501711	1552.731761	17.719130
35.691434	1532.749382	17.724147
35.606046	1551.495734	17.729165
35.804148	1550.380725	17.734183
35.802698	1550.980637	17.739200
35.838553	1546.384644	17.744218
35.924320	1553.200779	17.749235
35.834852	1567.927776	17.754253
35.963678	1569.438001	17.759271
36.113514	1578.329354	17.764288
36.235256	1576.865178	17.769306
36.590489	1568.492692	17.774323
36.209909	1577.007702	17.779341
36.246397	1563.483301	17.784359
36.120902	1569.670256	17.789376
36.088930	1571.244902	17.794394
36.526963	1565.897667	17.799411
36.322239	1557.910425	17.804429
36.261706	1560.357116	17.809447
36.247637	1569.237415	17.814464
36.075761	1565.358880	17.819482
36.620967	1557.671869	17.824499
36.539065	1562.526808	17.829517
36.259678	1568.515624	17.834535
36.379508	1563.572652	17.839552
36.322552	1565.062852	17.844570
36.469288	1571.000008	17.849587
36.568497	1588.693403	17.854605
36.799803	1588.599661	17.859623
36.842859	1593.817775	17.864640
37.128296	1588.222180	17.869658
37.143654	1590.772844	17.874675
36.974039	1586.336452	17.879693
36.797434	1575.914635	17.884711
37.088595	1588.426274	17.889728
37.373225	1577.040685	17.894746
37.092555	1564.566039	17.899763
36.982798	1556.791417	17.904781
37.360007	1569.002968	17.909799
37.047285	1563.328081	17.914816
36.885277	1564.264026	17.919834
37.289462	1572.265627	17.924851
37.058089	1581.700809	17.929869
37.415238	1585.091724	17.934887
37.214561	1581.810865	17.939904
37.305555	1587.722217	17.944922
37.215182	1579.907761	17.949939
37.069250	1588.685102	17.954957
37.447196	1584.476939	17.959975
37.796020	1588.370019	17.964992
37.777913	1581.688078	17.970010
37.383902	1578.986474	17.975027
37.190096	1578.046198	17.980045
37.374940	1580.762891	17.985063
37.090449	1578.541574	17.990080
37.108808	1580.690168	17.995098
37.843726	1596.406666	18.000115
37.630984	1609.811600	18.005133
37.706876	1610.549101	18.010151
37.762300	1607.229767	18.015168
38.173532	1610.934172	18.020186
38.116789	1609.231438	18.025203
38.099720	1614.048492	18.030221
38.000422	1601.902444	18.035239
37.979282	1609.380398	18.040256
38.357030	1608.983275	18.045274
38.169372	1615.943137	18.050291
38.024490	1616.114440	18.055309
37.754135	1608.733313	18.060327
38.390295	1599.377683	18.065344
37.954510	1612.145144	18.070362
38.380968	1606.489971	18.075379
38.055072	1608.658957	18.080397
38.285732	1615.922780	18.085415
38.062592	1616.386175	18.090432
38.305037	1628.430324	18.095450
38.463397	1638.437621	18.100467
38.129330	1639.278438	18.105485
38.756950	1648.601741	18.110503
38.781938	1644.852006	18.115520
38.417188	1646.589242	18.120538
38.859338	1647.446413	18.125555
38.712609	1643.721175	18.130573
38.875315	1634.710456	18.135591
39.003174	1634.501559	18.140608
38.795380	1631.799031	18.145626
39.122556	1629.600048	18.150643
38.625230	1640.921033	18.155661
38.957599	1631.490490	18.160679
38.904258	1632.603326	18.165696
39.020557	1642.897512	18.170714
39.273015	1632.758153	18.175731
38.945203	1634.638090	18.180749
39.009287	1633.501959	18.185767
39.250689	1637.882523	18.190784
39.125884	1639.194989	18.195802
39.052449	1634.409586	18.200819
39.110635	1635.832302	18.205837
39.232055	1638.685885	18.210855
39.457026	1648.513261	18.215872
39.517276	1652.229730	18.220890
39.423342	1645.982365	18.225907
39.601755	1643.462737	18.230925
39.540409	1647.457606	18.235943
39.958516	1649.041987	18.240960
39.738668	1645.471375	18.245978
40.021555	1645.021454	18.250995
39.849131	1648.663457	18.256013
40.140212	1640.900768	18.261031
40.185302	1632.197713	18.266048
39.702227	1634.037217	18.271066
39.731537	1625.650558	18.276083
39.676205	1621.172398	18.281101
39.942751	1617.745663	18.286119
39.799270	1625.674984	18.291136
39.791481	1625.996421	18.296154
40.017128	1641.815009	18.301171
39.711073	1647.393704	18.306189
39.808246	1639.798950	18.311207
39.848020	1636.600705	18.316224
39.581248	1647.698480	18.321242
39.732797	1640.608107	18.326259
39.751886	1651.854220	18.331277
39.999525	1676.117232	18.336295
40.202468	1664.167152	18.341312
39.881417	1676.844015	18.346330
40.417946	1670.844214	18.351347
40.264961	1676.913716	18.356365
40.385080	1672.812395	18.361383
40.411297	1678.995926	18.366400
40.449915	1692.852619	18.371418
40.568719	1693.612545	18.376435
40.578136	1709.628817	18.381453
40.725440	1701.321006	18.386471
41.040746	1691.288526	18.391488
41.030767	1699.709953	18.396506
41.319227	1689.544124	18.401523
40.789844	1679.925140	18.406541
40.901046	1671.798519	18.411559
41.311461	1683.447575	18.416576
40.862345	1679.101531	18.421594
41.135617	1667.716969	18.426611
41.185426	1680.878491	18.431629
41.250697	1682.726023	18.436647
41.064614	1660.195467	18.441664
40.554046	1678.181272	18.446682
41.020555	1672.426136	18.451699
41.311510	1690.043804	18.456717
41.092550	1693.095884	18.461735
41.526085	1687.570219	18.466752
41.215482	1693.657952	18.471770
41.018623	1690.960690	18.476787
41.460087	1691.911285	18.481805
41.459373	1685.338231	18.486823
41.611668	1682.860717	18.491840
41.326228	1685.573015	18.496858
41.658085	1697.650445	18.501875
41.833299	1714.964864	18.506893
41.827528	1720.835990	18.511911
42.101738	1723.656416	18.516928
41.813357	1709.143550	18.521946
41.700826	1695.683473	18.526963
42.142720	1713.520270	18.531981
41.866889	1712.194354	18.536999
42.183593	1708.334883	18.542016
42.045219	1718.089002	18.547034
42.575833	1703.845257	18.552051
42.255310	1694.034199	18.557069
41.989479	1684.890077	18.562087
42.186380	1678.909896	18.567104
42.203673	1688.094913	18.572122
42.100423	1687.670739	18.577139
42.291734	1697.813170	18.582157
42.074033	1706.607186	18.587175
42.526220	1704.068594	18.592192
42.323109	1714.030281	18.597210
42.309612	1701.957349	18.602227
42.342133	1713.256007	18.607245
42.446742	1705.239122	18.612263
42.628263	1712.679238	18.617280
42.493953	1715.318485	18.622298
42.693324	1708.467015	18.627315
42.630455	1704.247953	18.632333
42.666183	1716.744511	18.637351
42.396790	1708.213173	18.642368
42.226518	1712.735546	18.647386
42.676732	1722.431972	18.652403
43.033119	1732.417170	18.657421
42.451572	1739.017503	18.662439
43.094323	1737.874918	18.667456
43.025948	1739.127654	18.672474
42.811594	1739.661251	18.677491
43.036810	1731.909423	18.682509
43.134658	1740.194907	18.687527
43.390325	1739.867208	18.692544
43.222351	1741.225807	18.697562
43.038089	1731.873268	18.702579
43.230530	1733.608804	18.707597
42.809365	1741.104239	18.712615
43.195319	1755.071192	18.717632
43.549157	1759.991445	18.722650
43.607953	1773.246439	18.727667
43.904530	1767.686337	18.732685
43.994542	1771.903816	18.737703
44.106070	1753.403403	18.742720
43.582133	1745.083484	18.747738
43.639200	1734.177196	18.752755
43.360402	1733.835238	18.757773
43.168628	1755.631751	18.762791
43.345887	1747.212655	18.767808
43.546156	1762.913521	18.772826
43.550209	1757.725877	18.777843
43.905059	1760.797525	18.782861
44.015902	1785.101469	18.787879
44.438225	1778.080766	18.792896
44.291458	1790.665083	18.797914
44.436553	1783.478075	18.802931
44.573083	1755.790377	18.807949
44.333799	1762.849011	18.812967
44.341156	1747.555246	18.817984
44.199349	1752.942214	18.823002
44.014093	1755.296595	18.828019
44.355337	1762.405562	18.833037
44.326249	1775.866844	18.838055
44.525396	1776.692212	18.843072
44.732623	1780.257997	18.848090
44.573433	1779.463946	18.853107
44.565861	1775.310513	18.858125
44.630568	1778.972337	18.863143
44.525024	1773.094562	18.868160
44.836601	1777.330080	18.873178
44.742428	1779.092607	18.878195
44.554881	1782.048557	18.883213
44.529941	1778.385798	18.888231
45.223843	1780.097362	18.893248
44.732720	1777.529125	18.898266
44.816444	1781.709459	18.903283
45.174971	1795.472721	18.908301
45.144329	1799.493648	18.913319
45.227324	1807.965094	18.918336
45.067873	1818.086943	18.923354
45.075833	1820.371151	18.928371
45.194352	1807.540049	18.933389
45.408516	1809.843262	18.938407
45.658929	1806.003800	18.943424
45.676784	1807.961955	18.948442
45.469967	1810.779761	18.953459
46.051667	1804.913771	18.958477
45.678474	1799.334243	18.963495
45.762579	1801.024339	18.968512
45.737485	1799.826977	18.973530
45.739103	1796.414937	18.978547
45.926511	1791.754407	18.983565
45.755077	1793.886030	18.988583
45.716550	1789.767246	18.993600
45.756971	1797.068167	18.998618
45.504060	1794.482137	19.003635
45.950097	1790.753595	19.008653
45.819739	1799.517847	19.013671
45.861109	1796.771277	19.018688
45.690417	1803.838651	19.023706
45.855682	1794.467570	19.028723
46.085764	1797.203582	19.033741
45.703882	1805.744522	19.038759
46.164599	1821.859807	19.043776
46.033513	1833.002176	19.048794
46.234863	1827.621602	19.053811
46.370184	1822.810630	19.058829
45.982861	1829.074900	19.063847
46.405607	1829.073082	19.068864
46.143035	1836.660808	19.073882
46.258200	1844.853716	19.078899
46.451228	1857.820805	19.083917
46.469916	1864.893070	19.088935
46.502360	1866.425583	19.093952
46.742401	1863.638625	19.098970
46.756358	1864.169461	19.103987
47.112205	1851.073433	19.109005
46.809903	1855.089750	19.114023
47.080983	1856.287469	19.119040
46.989948	1852.336814	19.124058
46.440383	1857.645663	19.129075
46.868743	1862.850464	19.134093
47.017829	1885.009621	19.139111
47.503332	1882.386350	19.144128
47.597525	1877.082952	19.149146
47.372569	1883.467999	19.154163
47.764613	1871.644325	19.159181
47.468504	1878.710058	19.164199
47.707760	1863.087226	19.169216
47.816509	1848.481307	19.174234
47.570470	1845.044908	19.179251
47.871212	1844.025483	19.184269
47.203339	1844.299921	19.189287
47.157371	1845.397772	19.194304
47.166356	1861.430808	19.199322
47.252480	1875.368382	19.204339
47.545142	1874.474311	19.209357
47.587205	1880.563565	19.214375
47.794045	1877.069887	19.219392
48.154611	1900.826357	19.224410
48.072623	1908.992888	19.229427
48.160732	1903.979862	19.234445
48.302791	1907.773400	19.239463
48.249730	1901.762474	19.244480
47.957846	1890.309910	19.249498
48.256177	1902.509589	19.254515
48.287386	1907.508901	19.259533
48.277332	1907.116534	19.264551
48.266857	1907.999061	19.269568
48.652838	1901.538660	19.274586
48.462107	1900.702581	19.279603
48.528356	1896.290825	19.284621
48.308587	1899.598988	19.289639
48.820176	1897.630067	19.294656
48.905500	1901.302286	19.299674
48.143827	1896.392175	19.304691
48.440408	1896.257702	19.309709
48.548938	1897.289817	19.314727
48.482193	1894.157977	19.319744
48.727444	1893.363882	19.324762
48.662940	1907.879190	19.329779
48.999059	1924.680579	19.334797
48.775291	1925.755119	19.339815
48.728391	1927.307863	19.344832
49.233481	1921.478925	19.349850
48.590640	1930.048574	19.354867
48.890170	1921.622919	19.359885
48.973717	1932.130990	19.364903
49.392017	1945.893150	19.369920
49.404903	1954.104233	19.374938
49.144083	1960.622811	19.379955
49.518105	1956.662449	19.384973
49.836226	1961.519388	19.389991
49.707623	1958.053281	19.395008
49.599585	1959.776785	19.400026
49.694003	1957.960398	19.405043
49.895084	1954.906642	19.410061
50.023149	1952.167344	19.415079
49.963051	1950.121026	19.420096
50.270281	1950.437160	19.425114
49.982089	1945.182094	19.430131
50.197499	1941.780291	19.435149
49.792695	1949.010513	19.440167
49.856828	1944.936896	19.445184
50.054432	1934.716659	19.450202
50.126396	1947.472762	19.455219
50.160934	1946.153702	19.460237
50.026870	1948.729955	19.465255
50.293981	1941.601413	19.470272
50.226005	1940.013102	19.475290
50.499392	1946.333375	19.480307
50.203765	1931.936463	19.485325
50.335029	1941.568121	19.490343
50.235391	1945.866264	19.495360
50.542845	1958.278653	19.500378
50.478934	1968.705258	19.505395
50.620889	1975.529993	19.510413
50.816215	1973.545712	19.515431
50.854162	1970.567784	19.520448
50.870414	1970.172241	19.525466
50.594728	1974.343633	19.530483
50.908645	1962.935197	19.535501
50.913026	1971.918185	19.540519
50.698140	1958.894915	19.545536
51.228707	1973.138914	19.550554
51.287953	1994.005202	19.555571
51.025337	1990.807347	19.560589
51.448708	1985.733664	19.565607
51.247278	1990.581756	19.570624
51.473604	1997.107485	19.575642
51.504921	2001.305611	19.580659
51.688446	1997.117326	19.585677
51.379460	1993.712971	19.590695
51.347376	2001.829554	19.595712
51.779116	1993.641816	19.600730
51.502247	2000.241022	19.605747
51.798046	2003.214228	19.610765
51.696354	1992.450584	19.615783
51.672674	2005.369819	19.620800
51.783442	1992.809932	19.625818
51.823384	1998.288941	19.630835
51.782211	1994.031561	19.635853
51.802571	1988.048997	19.640871
51.855037	1997.508694	19.645888
51.979627	1992.703778	19.650906
52.081709	2001.275321	19.655923
51.995935	2012.943792	19.660941
52.520823	2011.885669	19.665959
51.916721	2022.639949	19.670976
52.151383	2008.247289	19.675994
52.347705	2016.872923	19.681011
52.252154	2016.890389	19.686029
52.068213	2016.601616	19.691047
51.959167	2026.863289	19.696064
52.500225	2023.942994	19.701082
52.556924	2042.931379	19.706099
52.643420	2045.148284	19.711117
52.719936	2036.661066	19.716135
52.484994	2034.572820	19.721152
52.832016	2031.359447	19.726170
52.467719	2041.611030	19.731187
52.926337	2040.528444	19.736205
52.856927	2047.170092	19.741223
52.900884	2052.942557	19.746240
53.241354	2052.005127	19.751258
53.434343	2060.582124	19.756275
53.567197	2065.256774	19.761293
53.646620	2067.032323	19.766311
53.404033	2056.756149	19.771328
53.617683	2054.115658	19.776346
53.631938	2045.905285	19.781363
53.663340	2049.019918	19.786381
53.779101	2041.970329	19.791399
53.564637	2058.909881	19.796416
54.127460	2051.716970	19.801434
53.737405	2049.338649	19.806451
53.872451	2033.794714	19.811469
54.004148	2045.005143	19.816487
53.781577	2046.807857	19.821504
54.151708	2041.425248	19.826522
53.902344	2043.967850	19.831539
54.310785	2054.192282	19.836557
54.139295	2049.702128	19.841575
53.935735	2055.221082	19.846592
54.218524	2044.754379	19.851610
54.181519	2045.978716	19.856627
54.186988	2046.935778	19.861645
54.346736	2044.022316	19.866663
54.132718	2043.705451	19.871680
54.331693	2039.388217	19.876698
54.334452	2046.363987	19.881715
54.506769	2049.595842	19.886733
54.751366	2065.111717	19.891751
54.515310	2077.142137	19.896768
54.722580	2079.387870	19.901786
54.999755	2079.021564	19.906803
54.871433	2081.819728	19.911821
55.002845	2077.203031	19.916839
54.779404	2084.148947	19.921856
54.912684	2075.744437	19.926874
55.039834	2079.817658	19.931891
55.035854	2075.959621	19.936909
55.167955	2069.980177	19.941927
54.926173	2081.757998	19.946944
54.863583	2076.789556	19.951962
54.966447	2082.905437	19.956979
54.944620	2100.987973	19.961997
55.488185	2095.878211	19.967015
55.280739	2103.457726	19.972032
55.396754	2092.517016	19.977050
55.612801	2098.363368	19.982067
55.502870	2106.137768	19.987085
55.809964	2104.442847	19.992103
55.183845	2102.624880	19.997120
55.460216	2116.233522	20.002138
55.686427	2131.869047	20.007155
55.509246	2135.678885	20.012173
55.840983	2127.256841	20.017191
55.596831	2138.477994	20.022208
55.588605	2128.301161	20.027226
56.251468	2146.501882	20.032243
56.212346	2157.627681	20.037261
56.545801	2155.213013	20.042279
56.105654	2167.186347	20.047296
56.571218	2154.320725	20.052314
56.566629	2160.314267	20.057331
56.733967	2164.397392	20.062349
56.772795	2152.116621	20.067367
57.004208	2153.176834	20.072384
56.940605	2137.625528	20.077402
56.647114	2114.874686	20.082419
56.528640	2126.664015	20.087437
57.007306	2139.861218	20.092455
56.908149	2151.397753	20.097472
56.665422	2149.935603	20.102490
57.123453	2153.587510	20.107507
57.042948	2148.340112	20.112525
57.166403	2145.897616	20.117543
57.235242	2153.827877	20.122560
57.418976	2145.825225	20.127578
57.365751	2145.159282	20.132595
57.245928	2149.425782	20.137613
57.354125	2143.956190	20.142631
57.209869	2142.197019	20.147648
57.058060	2145.825093	20.152666
57.176787	2153.734101	20.157683
57.418594	2171.570698	20.162701
57.736009	2166.678681	20.167719
57.371299	2167.336402	20.172736
57.752994	2179.837862	20.177754
58.019397	2165.509882	20.182771
57.604884	2167.653457	20.187789
58.117914	2166.095697	20.192807
58.069068	2176.968387	20.197824
58.091283	2174.235159	20.202842
58.117591	2169.444887	20.207859
57.784804	2176.256582	20.212877
58.217800	2181.177250	20.217895
58.308620	2193.109540	20.222912
58.468051	2187.494436	20.227930
58.582876	2188.244417	20.232947
58.869979	2190.701759	20.237965
58.963717	2188.328352	20.242983
58.838856	2187.154567	20.248000
59.064375	2172.599090	20.253018
59.070275	2156.322454	20.258035
58.772538	2161.360960	20.263053
59.022560	2149.536182	20.268071
59.072924	2157.401392	20.273088
58.857441	2160.251799	20.278106
58.938939	2145.496171	20.283123
59.033620	2152.853632	20.288141
59.433123	2165.161574	20.293159
59.281441	2173.694913	20.298176
58.723545	2174.029492	20.303194
59.279089	2170.876056	20.308211
58.699332	2182.969372	20.313229
59.030530	2186.531654	20.318247
58.697074	2188.934655	20.323264
59.306822	2197.077354	20.328282
59.400764	2208.424866	20.333299
59.383711	2219.593120	20.338317
59.659121	2212.028420	20.343335
59.637935	2217.023121	20.348352
59.790001	2213.640804	20.353370
59.820212	2207.402185	20.358387
59.703114	2209.768577	20.363405
59.911040	2207.203419	20.368423
59.771362	2209.665679	20.373440
59.772991	2221.541496	20.378458
60.127247	2230.985225	20.383475
60.040245	2241.000466	20.388493
59.997470	2239.166998	20.393511
60.054283	2246.508331	20.398528
60.205578	2235.049062	20.403546
60.353671	2230.672086	20.408563
59.831071	2233.639896	20.413581
60.257815	2257.926133	20.418599
60.751209	2265.723948	20.423616
60.736385	2262.992113	20.428634
60.803369	2263.213384	20.433651
60.636830	2262.370916	20.438669
60.938107	2263.444766	20.443687
60.996100	2253.374608	20.448704
60.787287	2254.724657	20.453722
61.278028	2251.240584	20.458739
61.113521	2263.261662	20.463757
61.020208	2259.243561	20.468775
61.177945	2261.618393	20.473792
61.302738	2275.647958	20.478810
61.742371	2275.308688	20.483827
61.755352	2288.479579	20.488845
61.661740	2283.637865	20.493863
61.765618	2269.092203	20.498880
61.629312	2265.485565	20.503898
61.861213	2265.179510	20.508915
61.628702	2271.823849	20.513933
61.697810	2266.914645	20.518951
61.788300	2277.117459	20.523968
61.783295	2271.306315	20.528986
61.753924	2269.569446	20.534003
61.844752	2278.622553	20.539021
62.122669	2272.049574	20.544039
62.077195	2272.072922	20.549056
62.171593	2275.079528	20.554074
62.214495	2273.525976	20.559091
62.314794	2292.463351	20.564109
62.657475	2292.029893	20.569127
62.397624	2304.703430	20.574144
62.576698	2299.942944	20.579162
63.252657	2297.706592	20.584179
62.976424	2300.761973	20.589197
62.863103	2278.272016	20.594215
62.932181	2267.031856	20.599232
62.525680	2270.408812	20.604250
62.717130	2285.160449	20.609267
62.959153	2301.406938	20.614285
62.637616	2293.709533	20.619303
62.739803	2304.046654	20.624320
62.982236	2305.005049	20.629338
63.251556	2291.371381	20.634355
62.982080	2307.784857	20.639373
63.240052	2318.680469	20.644391
63.559514	2322.819554	20.649408
63.201900	2339.173243	20.654426
63.512367	2327.287139	20.659443
63.438455	2330.221620	20.664461
63.485159	2329.604481	20.669479
63.840446	2322.510775	20.674496
63.841970	2336.141890	20.679514
64.158389	2328.950675	20.684531
63.626708	2330.035672	20.689549
63.843384	2322.829871	20.694567
64.058045	2326.329195	20.699584
63.572595	2325.604097	20.704602
63.919195	2322.744688	20.709619
63.870536	2348.957502	20.714637
63.982340	2342.173011	20.719655
64.326694	2349.096688	20.724672
64.054880	2348.642528	20.729690
64.230067	2345.947724	20.734707
64.363896	2358.087202	20.739725
64.374749	2355.032187	20.744743
64.574164	2374.617454	20.749760
64.357567	2379.465027	20.754778
64.680386	2379.478183	20.759795
64.894262	2384.806476	20.764813
64.841986	2375.684067	20.769831
65.300740	2380.824168	20.774848
64.986333	2376.985564	20.779866
65.353105	2370.352160	20.784883
65.190836	2370.366892	20.789901
65.331997	2368.847063	20.794919
65.014999	2360.324033	20.799936
64.988248	2379.488859	20.804954
65.155944	2381.130531	20.809971
65.282088	2398.538094	20.814989
65.619512	2393.643481	20.820007
65.781543	2393.027718	20.825024
65.929397	2407.514236	20.830042
65.925894	2393.368540	20.835059
66.013310	2403.449104	20.840077
65.609962	2399.169294	20.845095
65.866781	2388.859031	20.850112
65.881813	2395.095488	20.855130
65.900267	2385.627095	20.860147
65.656672	2402.678541	20.865165
66.078885	2400.371193	20.870183
66.240772	2404.438748	20.875200
66.312589	2422.530169	20.880218
66.598146	2409.494528	20.885235
66.418859	2419.986604	20.890253
66.771170	2419.642498	20.895271
66.702682	2417.864843	20.900288
66.570407	2424.406426	20.905306
66.912230	2418.272827	20.910323
66.802619	2420.447844	20.915341
66.669296	2419.012830	20.920359
66.971451	2423.875710	20.925376
66.926199	2426.111728	20.930394
66.965351	2444.909800	20.935411
66.926799	2443.052772	20.940429
66.952390	2453.380626	20.945447
67.300530	2446.604205	20.950464
67.115205	2457.952074	20.955482
67.331307	2446.839417	20.960499
67.441796	2450.023718	20.965517
67.355337	2449.326255	20.970535
67.443015	2438.286053	20.975552
67.656442	2449.082827	20.980570
67.994104	2465.518388	20.985587
67.879492	2477.502234	20.990605
67.633351	2474.812206	20.995623
68.170113	2465.084708	21.000640
68.166787	2461.830041	21.005658
68.005972	2454.854014	21.010675
68.344533	2458.768703	21.015693
68.212673	2463.086102	21.020711
68.331492	2460.664405	21.025728
68.225665	2463.482929	21.030746
68.491107	2454.144081	21.035763
68.418038	2471.103583	21.040781
68.283423	2462.056965	21.045799
68.167887	2455.032494	21.050816
68.774071	2451.091053	21.055834
68.410277	2458.615127	21.060851
68.490018	2470.123457	21.065869
68.488337	2491.161926	21.070887
68.718736	2484.217967	21.075904
68.763468	2492.648876	21.080922
68.972272	2498.656037	21.085939
69.117420	2486.635759	21.090957
69.007508	2483.206600	21.095975
69.266839	2496.202617	21.100992
69.507545	2510.313995	21.106010
69.712433	2520.022016	21.111027
70.006103	2514.153454	21.116045
69.722717	2506.665386	21.121063
69.824303	2498.150142	21.126080
69.888354	2504.734846	21.131098
69.589460	2493.959803	21.136115
70.071749	2498.536961	21.141133
69.899823	2505.204440	21.146151
69.971836	2502.594807	21.151168
69.684614	2506.020964	21.156186
70.051520	2502.388434	21.161203
69.732667	2504.954033	21.166221
69.820574	2501.859064	21.171239
70.240278	2508.470320	21.176256
70.212842	2521.020506	21.181274
70.489865	2528.894834	21.186291
70.495243	2537.962241	21.191309
70.619512	2533.344230	21.196327
70.801675	2530.612805	21.201344
70.529949	2529.691669	21.206362
70.630995	2532.199953	21.211379
70.747240	2525.390237	21.216397
70.841700	2527.034995	21.221415
71.284073	2538.207333	21.226432
71.031718	2556.404163	21.231450
70.876172	2548.774034	21.236467
71.434663	2554.289434	21.241485
71.405205	2551.726910	21.246503
71.491833	2546.743059	21.251520
71.450972	2553.484533	21.256538
71.792041	2551.696928	21.261555
71.446954	2550.637535	21.266573
71.585776	2555.539706	21.271591
71.854449	2544.502139	21.276608
71.714066	2551.525066	21.281626
72.016717	2546.721601	21.286643
71.930867	2539.676822	21.291661
71.752264	2552.312302	21.296679
72.017596	2559.092062	21.301696
72.156149	2579.389673	21.306714
72.084370	2579.405564	21.311731
72.425538	2580.337392	21.316749
72.229818	2586.063120	21.321767
72.200598	2586.647590	21.326784
72.311982	2589.116767	21.331802
72.154763	2580.512826	21.336819
72.508938	2587.249933	21.341837
72.378789	2607.144800	21.346855
72.295987	2617.485198	21.351872
72.337710	2606.561153	21.356890
72.323862	2613.508823	21.361907
72.933527	2631.738218	21.366925
72.777092	2643.628717	21.371943
73.529773	2633.309424	21.376960
73.070885	2642.680941	21.381978
73.268065	2647.812864	21.386995
73.347461	2634.337125	21.392013
73.234762	2643.099319	21.397031
73.618067	2630.893426	21.402048
73.705916	2632.353451	21.407066
73.343049	2631.123364	21.412083
73.766074	2631.122687	21.417101
73.441297	2638.507700	21.422119
73.925305	2639.860792	21.427136
74.249491	2656.643690	21.432154
74.071854	2665.581226	21.437171
74.237618	2654.538179	21.442189
74.091942	2665.112654	21.447207
74.450429	2650.015786	21.452224
74.276067	2658.453926	21.457242
74.658500	2665.112368	21.462259
74.670837	2648.648313	21.467277
74.679942	2651.112387	21.472295
74.805719	2654.419403	21.477312
74.564964	2650.886665	21.482330
74.541844	2648.285278	21.487347
74.865201	2636.671627	21.492365
74.629401	2656.563576	21.497383
74.745203	2653.617906	21.502400
75.049916	2672.165575	21.507418
74.933736	2681.098851	21.512435
75.165738	2678.117007	21.517453
75.009512	2681.396306	21.522471
75.139280	2672.597149	21.527488
75.403504	2677.555765	21.532506
75.382286	2681.002487	21.537523
75.672088	2674.311617	21.542541
76.112621	2694.030210	21.547559
76.081191	2689.032001	21.552576
76.023480	2671.875536	21.557594
75.623943	2677.091701	21.562611
75.884636	2686.444107	21.567629
76.222351	2701.868819	21.572647
75.997290	2694.325331	21.577664
76.400339	2691.119087	21.582682
76.356923	2696.308579	21.587699
76.582679	2692.270215	21.592717
76.325557	2693.123541	21.597735
76.642027	2689.398526	21.602752
76.613222	2687.437880	21.607770
76.380126	2694.938851	21.612787
76.868503	2677.565969	21.617805
76.683752	2687.710681	21.622823
76.975349	2689.146033	21.627840
77.107458	2697.849219	21.632858
76.794041	2709.695676	21.637875
76.915862	2707.199424	21.642893
76.748340	2714.200144	21.647911
77.120589	2713.018030	21.652928
77.187891	2709.259457	21.657946
77.136451	2717.678851	21.662963
77.601164	2723.407491	21.667981
77.325781	2747.782008	21.672999
77.699888	2737.091048	21.678016
77.746653	2737.662548	21.683034
77.585794	2737.435297	21.688051
77.736714	2736.132336	21.693069
77.691786	2738.511269	21.698087
77.736796	2734.088225	21.703104
77.810499	2734.981272	21.708122
77.765289	2745.759262	21.713139
78.216471	2762.746067	21.718157
78.128291	2755.080665	21.723175
78.547537	2764.650584	21.728192
78.520830	2763.339234	21.733210
78.571160	2755.639480	21.738227
78.744162	2752.450446	21.743245
78.578637	2757.378267	21.748263
78.371269	2753.317500	21.753280
78.773531	2761.835431	21.758298
78.739872	2766.272491	21.763315
78.910037	2775.354487	21.768333
78.905855	2784.557487	21.773351
79.219967	2792.065153	21.778368
79.571977	2788.392108	21.783386
79.242918	2785.984671	21.788403
79.642645	2783.040001	21.793421
79.526825	2785.682666	21.798439
79.278555	2789.699328	21.803456
79.416129	2777.049720	21.808474
79.654206	2792.615438	21.813491
79.336618	2803.441323	21.818509
79.686668	2811.348983	21.823527
79.689116	2805.084797	21.828544
80.261025	2797.968004	21.833562
80.019764	2810.817232	21.838579
80.191664	2804.197407	21.843597
80.150458	2815.285435	21.848615
80.207780	2829.520387	21.853632
80.650590	2828.906547	21.858650
80.720624	2828.344979	21.863667
80.532355	2825.317723	21.868685
80.880310	2820.140112	21.873703
80.987031	2825.220531	21.878720
80.878627	2819.176284	21.883738
80.889389	2813.070573	21.888755
80.871389	2818.336613	21.893773
80.705244	2821.968792	21.898791
81.064695	2827.117217	21.903808
81.390731	2846.221842	21.908826
81.287940	2862.605545	21.913843
81.588079	2861.633800	21.918861
81.641592	2850.388711	21.923879
81.483385	2853.471902	21.928896
81.534526	2856.981885	21.933914
81.423908	2854.292187	21.938931
81.753495	2852.391875	21.943949
82.119987	2850.064160	21.948967
81.769544	2849.753721	21.953984
82.032301	2853.442068	21.959002
81.715582	2873.787489	21.964019
81.916392	2876.303721	21.969037
81.842586	2881.616821	21.974055
81.710063	2879.268961	21.979072
82.040201	2895.030973	21.984090
82.407872	2909.094918	21.989107
82.741131	2905.141464	21.994125
82.864529	2906.003062	21.999143
82.858602	2908.283824	22.004160
82.955565	2902.320118	22.009178
82.822473	2904.659338	22.014195
83.040296	2909.782811	22.019213
82.803115	2904.644176	22.024231
82.973018	2917.956559	22.029248
83.302184	2928.817977	22.034266
83.177144	2928.205233	22.039283
83.314426	2930.352434	22.044301
83.699903	2923.502299	22.049319
83.287813	2924.747466	22.054336
83.263514	2924.888184	22.059354
83.764741	2933.677643	22.064371
84.091590	2952.515707	22.069389
84.402258	2950.268487	22.074407
84.161829	2946.859259	22.079424
84.282953	2933.309025	22.084442
83.867976	2939.565713	22.089459
84.173026	2942.321805	22.094477
84.301175	2947.147514	22.099495
84.128624	2951.232002	22.104512
84.685219	2938.640061	22.109530
84.766588	2951.203289	22.114547
84.670702	2943.090608	22.119565
84.656910	2944.530482	22.124583
84.642547	2951.619344	22.129600
84.816064	2966.475393	22.134618
84.779742	2980.047977	22.139635
85.001423	2973.909250	22.144653
85.127793	2967.080735	22.149671
84.963317	2971.048133	22.154688
85.424375	2967.998779	22.159706
85.404599	2979.781859	22.164723
85.263321	3000.898859	22.169741
85.700308	3002.750364	22.174759
85.303276	3000.945930	22.179776
85.607075	2996.991425	22.184794
85.573420	3008.437032	22.189811
85.868939	3005.548162	22.194829
85.855022	3018.659157	22.199847
86.136014	3027.894618	22.204864
86.592693	3031.166614	22.209882
86.548789	3030.714857	22.214899
86.587455	3024.746188	22.219917
86.756396	3018.793751	22.224935
86.506456	3020.221151	22.229952
86.579657	3021.882082	22.234970
87.106975	3021.770824	22.239987
86.635266	3015.750036	22.245005
87.151734	3014.857436	22.250023
86.788019	3025.393053	22.255040
87.146558	3013.764636	22.260058
87.157553	3027.398725	22.265075
87.225512	3039.232683	22.270093
87.601701	3043.278706	22.275111
87.130381	3042.727229	22.280128
87.620349	3046.908364	22.285146
87.820126	3045.261827	22.290163
87.526994	3046.435727	22.295181
87.552122	3049.498446	22.300199
87.785541	3045.033488	22.305216
87.770191	3048.515543	22.310234
87.789085	3067.720512	22.315251
88.026291	3068.681004	22.320269
88.540807	3069.157746	22.325287
88.096752	3070.025111	22.330304
88.583890	3072.757378	22.335322
88.761095	3073.103338	22.340339
88.231213	3081.230457	22.345357
88.815929	3072.930210	22.350375
88.604079	3078.830457	22.355392
88.650030	3076.493178	22.360410
88.771898	3098.177031	22.365427
88.903588	3102.426165	22.370445
88.959187	3105.244850	22.375463
89.043121	3113.285317	22.380480
89.141620	3108.826143	22.385498
89.264705	3108.255782	22.390515
89.078897	3105.630463	22.395533
89.199802	3111.870153	22.400551
89.249910	3127.472840	22.405568
89.707136	3126.421524	22.410586
89.753853	3131.216674	22.415603
89.870284	3134.667874	22.420621
90.080453	3122.382381	22.425639
89.639008	3126.624438	22.430656
89.371512	3133.279658	22.435674
89.748056	3156.247141	22.440691
89.683088	3161.239550	22.445709
90.425065	3158.641334	22.450727
90.422433	3180.167158	22.455744
90.262898	3179.509716	22.460762
90.550099	3178.075090	22.465779
90.554587	3176.692392	22.470797
90.774430	3176.539908	22.475815
90.453190	3180.109651	22.480832
90.802263	3197.187467	22.485850
91.572567	3211.952421	22.490867
91.385928	3211.857789	22.495885
91.760109	3204.928292	22.500903
91.598833	3208.183338	22.505920
91.528152	3199.187523	22.510938
91.820966	3196.904244	22.515955
91.800335	3203.922204	22.520973
91.818291	3197.123745	22.525991
91.811729	3196.539410	22.531008
91.900869	3193.186201	22.536026
91.892330	3196.554552	22.541043
91.794790	3204.334533	22.546061
92.359370	3205.514086	22.551079
92.321851	3220.899856	22.556096
92.246020	3222.256710	22.561114
92.379134	3224.990923	22.566131
92.156749	3228.029690	22.571149
92.454091	3225.585011	22.576167
92.696551	3244.746094	22.581184
92.837060	3253.497024	22.586202
92.727818	3254.132173	22.591219
92.899044	3249.191972	22.596237
93.201729	3248.540684	22.601255
93.333233	3259.455140	22.606272
93.112265	3256.517868	22.611290
93.568877	3271.400571	22.616307
93.450098	3283.295951	22.621325
93.976627	3273.888582	22.626343
93.748623	3274.913906	22.631360
93.835803	3274.532180	22.636378
93.929834	3280.355083	22.641395
94.092102	3281.015759	22.646413
94.180443	3267.713996	22.651431
94.146118	3269.329364	22.656448
94.168790	3273.882451	22.661466
94.433073	3280.393381	22.666483
94.400356	3298.388154	22.671501
94.597698	3302.355971	22.676519
94.685645	3302.407234	22.681536
94.698942	3306.813836	22.686554
94.718201	3302.188181	22.691571
94.320720	3308.046799	22.696589
94.834948	3309.309115	22.701607
94.996081	3315.837139	22.706624
95.043179	3327.073525	22.711642
95.424035	3320.886259	22.716659
95.348179	3335.993026	22.721677
95.617951	3325.897744	22.726695
95.408894	3329.146944	22.731712
95.541115	3319.523701	22.736730
95.580522	3324.235073	22.741747
95.647573	3332.987185	22.746765
96.055940	3340.291302	22.751783
96.154045	3351.743300	22.756800
95.968445	3350.704692	22.761818
96.078348	3345.876200	22.766835
96.021477	3347.206695	22.771853
96.210895	3344.368405	22.776871
96.210484	3349.771491	22.781888
96.811018	3360.920994	22.786906
96.799516	3366.864170	22.791923
96.583569	3381.187788	22.796941
96.723285	3374.562027	22.801959
96.687060	3373.314413	22.806976
96.889916	3376.266657	22.811994
96.814523	3387.163485	22.817011
96.875248	3401.992556	22.822029
97.017850	3399.606152	22.827047
97.451354	3407.100649	22.832064
97.356454	3408.324834	22.837082
97.436318	3421.263535	22.842099
97.554977	3438.251798	22.847117
97.860068	3438.114336	22.852135
97.764940	3434.899471	22.857152
97.792811	3437.316856	22.862170
98.179295	3443.023675	22.867187
98.165366	3462.529084	22.872205
98.372353	3465.604692	22.877223
98.350981	3466.091034	22.882240
98.416150	3472.911028	22.887258
99.008407	3457.386052	22.892275
98.785848	3458.123445	22.897293
98.927716	3456.851062	22.902311
98.995470	3460.393474	22.907328
98.680498	3483.146367	22.912346
99.250864	3478.147097	22.917363
99.214129	3493.617267	22.922381
99.233249	3483.142862	22.927399
99.662092	3483.993297	22.932416
99.520472	3480.417967	22.937434
99.754970	3476.576798	22.942451
99.500720	3500.452078	22.947469
99.951472	3499.364799	22.952487
99.965557	3504.171767	22.957504
99.662596	3505.854474	22.962522
100.071926	3512.991171	22.967539
100.250877	3512.621413	22.972557
100.391215	3503.782240	22.977575
100.488038	3520.689946	22.982592
100.714052	3528.907521	22.987610
101.270583	3528.454379	22.992627
101.016872	3532.215012	22.997645
101.238935	3526.166963	23.002663
100.993382	3526.497093	23.007680
100.932870	3527.761268	23.012698
101.382463	3523.810844	23.017715
101.080261	3533.110484	23.022733
101.402139	3527.640468	23.027751
101.279588	3530.411946	23.032768
101.324946	3533.762389	23.037786
101.467355	3522.265062	23.042803
101.397745	3547.838791	23.047821
101.318331	3551.111460	23.052839
101.286850	3553.517821	23.057856
101.354006	3561.636109	23.062874
101.775399	3565.012106	23.067891
101.600580	3588.453451	23.072909
101.893872	3587.385937	23.077927
102.262620	3592.870129	23.082944
102.439115	3606.113496	23.087962
102.756245	3605.767715	23.092979
102.836476	3610.661020	23.097997
102.978271	3608.227862	23.103015
102.899849	3607.764084	23.108032
102.989257	3610.712320	23.113050
103.225365	3592.636796	23.118067
103.513298	3603.201931	23.123085
103.686111	3600.178920	23.128103
104.010972	3589.718792	23.133120
103.560162	3594.538184	23.138138
104.154198	3600.265035	23.143155
104.308588	3602.670948	23.148173
103.754960	3597.109219	23.153191
104.290300	3594.971974	23.158208
104.229070	3614.863405	23.163226
104.321960	3612.218631	23.168243
104.231248	3622.081414	23.173261
104.441840	3618.430019	23.178279
104.291148	3621.577085	23.183296
104.391082	3620.379357	23.188314
104.701622	3622.209744	23.193331
104.530048	3623.667141	23.198349
104.910045	3639.064520	23.203367
104.862414	3647.282183	23.208384
104.822524	3653.498312	23.213402
105.059145	3649.958757	23.218419
104.754354	3652.645454	23.223437
104.931897	3667.654280	23.228455
105.297447	3670.976546	23.233472
105.350480	3677.212343	23.238490
105.222546	3696.110067	23.243507
105.179567	3701.106094	23.248525
105.466577	3713.871746	23.253543
105.933348	3722.026723	23.258560
105.973101	3732.117614	23.263578
106.085825	3733.868153	23.268595
106.446406	3721.441526	23.273613
106.385803	3731.610457	23.278631
106.822921	3733.028904	23.283648
106.958921	3754.053366	23.288666
107.167450	3748.429971	23.293683
107.367346	3753.653555	23.298701
107.497446	3762.887268	23.303719
107.823685	3741.737970	23.308736
107.542198	3732.230614	23.313754
107.777521	3715.673784	23.318771
107.332379	3711.890352	23.323789
107.504815	3728.103391	23.328807
107.607166	3732.016958	23.333824
107.540066	3741.983008	23.338842
107.763864	3740.814770	23.343859
107.601273	3743.167660	23.348877
107.618337	3756.699398	23.353895
108.202773	3762.800784	23.358912
107.939327	3774.916184	23.363930
108.156961	3774.157681	23.368947
108.437732	3779.640756	23.373965
108.230227	3797.578415	23.378983
108.622135	3808.020161	23.384000
108.531704	3811.713269	23.389018
108.663524	3804.786231	23.394035
108.756041	3818.657546	23.399053
108.498336	3822.551998	23.404071
109.127926	3818.291347	23.409088
109.115706	3838.717148	23.414106
109.272851	3832.330863	23.419123
109.575555	3846.367037	23.424141
109.521697	3855.086697	23.429159
110.098910	3855.236903	23.434176
110.010829	3860.312899	23.439194
110.077005	3850.943213	23.444211
110.159180	3858.318513	23.449229
110.011393	3858.172161	23.454247
110.676304	3849.203810	23.459264
110.418640	3848.725994	23.464282
110.363696	3856.698092	23.469299
110.822280	3866.432676	23.474317
110.531540	3881.783451	23.479335
111.156991	3883.645601	23.484352
110.952552	3886.247208	23.489370
111.112814	3882.318218	23.494387
111.093686	3877.647560	23.499405
110.927586	3903.652471	23.504423
111.481380	3905.803694	23.509440
111.413185	3912.482551	23.514458
111.566297	3909.977779	23.519475
111.839654	3915.061284	23.524493
111.624462	3913.062829	23.529511
112.366431	3928.326538	23.534528
112.297073	3934.695710	23.539546
112.355219	3925.373378	23.544563
112.304144	3925.728411	23.549581
112.263521	3930.342176	23.554599
112.680940	3920.963908	23.559616
112.564961	3934.657216	23.564634
112.713773	3951.107502	23.569651
113.135191	3946.835607	23.574669
112.881579	3960.306413	23.579687
113.243398	3949.693056	23.584704
113.340949	3959.928090	23.589722
113.244856	3953.536825	23.594739
113.611376	3951.909840	23.599757
113.458759	3977.735843	23.604775
113.821641	3976.197659	23.609792
113.673232	3984.484160	23.614810
113.643921	3988.065206	23.619827
113.639458	3982.066694	23.624845
113.465907	3996.870934	23.629863
114.175404	4006.644785	23.634880
114.148397	4020.450623	23.639898
114.669134	4022.467944	23.644915
114.850490	4029.483151	23.649933
114.562407	4035.055380	23.654951
114.876923	4036.313812	23.659968
114.739884	4036.620866	23.664986
115.095264	4038.800233	23.670003
115.379493	4027.579102	23.675021
115.178265	4037.268288	23.680039
115.387643	4044.408803	23.685056
115.347560	4065.745558	23.690074
115.385635	4073.758673	23.695091
115.648805	4066.217161	23.700109
115.751243	4066.339662	23.705127
115.995744	4072.412794	23.710144
115.934518	4089.742225	23.715162
116.313954	4093.751762	23.720179
116.428718	4077.111347	23.725197
116.721742	4080.158658	23.730215
116.569729	4077.794548	23.735232
116.618673	4081.141365	23.740250
116.746227	4079.889416	23.745267
116.630351	4080.664694	23.750285
116.962808	4106.895713	23.755303
117.047088	4115.232747	23.760320
117.395202	4115.030277	23.765338
117.105226	4113.099304	23.770355
117.305244	4109.385364	23.775373
117.315648	4115.786293	23.780391
117.457857	4127.735574	23.785408
117.581265	4136.913520	23.790426
117.701112	4139.206713	23.795443
117.646996	4137.947824	23.800461
117.802621	4162.424465	23.805479
117.734660	4163.962016	23.810496
118.131017	4173.757104	23.815514
118.063560	4185.534022	23.820531
118.473638	4197.348441	23.825549
118.516417	4200.467133	23.830567
118.761371	4196.292903	23.835584
118.826308	4217.512460	23.840602
119.093788	4226.415383	23.845619
119.386718	4227.856963	23.850637
119.430335	4234.013819	23.855655
119.423674	4236.765839	23.860672
119.791206	4227.565756	23.865690
120.079186	4230.607632	23.870707
119.860415	4226.999227	23.875725
119.919115	4245.229598	23.880743
120.044978	4244.948943	23.885760
120.267726	4243.482763	23.890778
120.458239	4246.043846	23.895795
120.668276	4244.220655	23.900813
120.724578	4248.062435	23.905831
120.489529	4245.034770	23.910848
120.859924	4253.029183	23.915866
120.951738	4271.006817	23.920883
121.256477	4266.682489	23.925901
121.280442	4277.415822	23.930919
121.111018	4274.154414	23.935936
121.424467	4278.004817	23.940954
120.858115	4286.211828	23.945971
121.292250	4292.206397	23.950989
121.457227	4310.493277	23.956007
121.463467	4316.505934	23.961024
121.629439	4336.314985	23.966042
121.763758	4343.320007	23.971059
121.676208	4346.624114	23.976077
122.283051	4360.795468	23.981095
122.383566	4364.793764	23.986112
122.476041	4366.620575	23.991130
122.417862	4370.078906	23.996147
123.125553	4376.588157	24.001165
123.099917	4393.578115	24.006183
123.080557	4397.070190	24.011200
123.060254	4390.987515	24.016218
123.142892	4394.321733	24.021235
123.195473	4392.002456	24.026253
123.512719	4412.114961	24.031271
123.395417	4414.085977	24.036288
123.819209	4408.808665	24.041306
123.615877	4427.892222	24.046323
124.036526	4428.493633	24.051341
124.238758	4442.969887	24.056359
124.291515	4443.095104	24.061376
124.557723	4448.675725	24.066394
124.187954	4445.294667	24.071411
124.710060	4443.372535	24.076429
124.637916	4457.302785	24.081447
125.226089	4463.096296	24.086464
125.442589	4458.188780	24.091482
125.273192	4471.465733	24.096499
125.540645	4468.623381	24.101517
125.427431	4468.704410	24.106535
125.404073	4465.973996	24.111552
125.806679	4467.766011	24.116570
125.522531	4468.303764	24.121587
125.653528	4475.402326	24.126605
125.640826	4493.369166	24.131623
125.741299	4496.476790	24.136640
125.879090	4502.533105	24.141658
126.065204	4539.998210	24.146675
126.369344	4527.184158	24.151693
126.257992	4529.228232	24.156711
126.518969	4545.132915	24.161728
126.724457	4549.735254	24.166746
126.769921	4551.022524	24.171763
127.069682	4566.537271	24.176781
127.350005	4581.679591	24.181799
127.383730	4589.749606	24.186816
127.613969	4580.776024	24.191834
127.464377	4583.819536	24.196851
127.796045	4590.705365	24.201869
127.761214	4605.836882	24.206887
127.908305	4602.748241	24.211904
128.150842	4608.636045	24.216922
128.270147	4610.167049	24.221939
128.256424	4628.563427	24.226957
128.379889	4634.477256	24.231975
128.791947	4635.994446	24.236992
128.843082	4644.320710	24.242010
128.631661	4656.989698	24.247027
129.102094	4668.466860	24.252045
129.050427	4678.006456	24.257063
129.195595	4674.005345	24.262080
129.594471	4670.615112	24.267098
129.577256	4685.212191	24.272115
130.140051	4686.101163	24.277133
130.400166	4694.707877	24.282151
130.174390	4699.138306	24.287168
130.462010	4688.718663	24.292186
130.336973	4687.410042	24.297203
130.614708	4689.736243	24.302221
130.619376	4686.806625	24.307239
130.541975	4692.908880	24.312256
130.600903	4706.335666	24.317274
130.587848	4717.659007	24.322291
131.185365	4718.258712	24.327309
131.272307	4715.397374	24.332327
131.350158	4729.978754	24.337344
131.786477	4740.362188	24.342362
131.539456	4755.767609	24.347379
131.944116	4752.554390	24.352397
132.156916	4748.959468	24.357415
131.679376	4747.432770	24.362432
132.139288	4748.547483	24.367450
132.137175	4761.953708	24.372467
132.449359	4774.291171	24.377485
132.522699	4774.494889	24.382503
132.481080	4782.683798	24.387520
132.701151	4773.814960	24.392538
132.665304	4783.945820	24.397555
133.034333	4788.150214	24.402573
132.958067	4795.243069	24.407591
132.939295	4804.063766	24.412608
133.125646	4803.062709	24.417626
132.989708	4818.906586	24.422643
133.107834	4829.087589	24.427661
133.219461	4834.122959	24.432679
133.413724	4845.378203	24.437696
133.926027	4850.378744	24.442714
133.730842	4865.074759	24.447731
134.025278	4880.223695	24.452749
134.533565	4884.293224	24.457767
134.595068	4888.716310	24.462784
134.632319	4886.182131	24.467802
134.784510	4896.748957	24.472819
134.941297	4901.946199	24.477837
135.211394	4912.346241	24.482855
135.256891	4914.705412	24.487872
135.517602	4903.120549	24.492890
135.287149	4911.917285	24.497907
135.477409	4927.327658	24.502925
135.593091	4932.282844	24.507943
135.658949	4938.881270	24.512960
136.061028	4931.778651	24.517978
136.433898	4956.013431	24.522995
136.160856	4965.536298	24.528013
136.356106	4967.647014	24.533031
136.516520	4973.252427	24.538048
136.890143	4964.448631	24.543066
137.093705	4996.871501	24.548083
137.472070	5000.662507	24.553101
137.188935	5001.230824	24.558119
137.193422	5004.637178	24.563136
137.761268	4999.028670	24.568154
137.644851	5005.864432	24.573171
137.529229	5003.042878	24.578189
137.530676	5014.723163	24.583207
137.617462	5024.544836	24.588224
137.896495	5024.602669	24.593242
138.250719	5041.846252	24.598259
138.240010	5056.633189	24.603277
138.426967	5057.434770	24.608295
138.388818	5062.916362	24.613312
138.959958	5075.450612	24.618330
138.798265	5098.090281	24.623347
139.083721	5092.884477	24.628365
138.974305	5087.835407	24.633383
139.206570	5122.869318	24.638400
139.628188	5113.770029	24.643418
139.502464	5120.349056	24.648435
139.920977	5109.734199	24.653453
140.012045	5118.333693	24.658471
139.916027	5133.338021	24.663488
140.363452	5139.051916	24.668506
140.640660	5136.936339	24.673523
140.468983	5137.377521	24.678541
141.136205	5128.438394	24.683559
140.696794	5144.866029	24.688576
141.166718	5159.240344	24.693594
140.922006	5166.979503	24.698611
141.178674	5166.799252	24.703629
141.500670	5167.326458	24.708647
141.451124	5175.401108	24.713664
141.408038	5185.012047	24.718682
141.417154	5191.772763	24.723699
141.596775	5198.271342	24.728717
141.938092	5206.532535	24.733735
141.860497	5228.871789	24.738752
142.330061	5228.005750	24.743770
142.516268	5230.430670	24.748787
142.220012	5233.639563	24.753805
142.656678	5239.075685	24.758823
142.744600	5250.848152	24.763840
143.325173	5247.677381	24.768858
143.252086	5244.046196	24.773875
143.076046	5240.565157	24.778893
143.353587	5254.859574	24.783911
143.269478	5273.510934	24.788928
143.588761	5284.216538	24.793946
143.579607	5277.985184	24.798963
143.880797	5296.327843	24.803981
144.203316	5300.536925	24.808999
143.929142	5301.867725	24.814016
144.285410	5305.347430	24.819034
144.719952	5313.849999	24.824051
144.720631	5338.976317	24.829069
144.844037	5334.790410	24.834087
144.930856	5333.083582	24.839104
144.943308	5330.643222	24.844122
145.184886	5344.720789	24.849139
145.218792	5357.467072	24.854157
145.766023	5353.306290	24.859175
145.668594	5360.554907	24.864192
145.605032	5371.520063	24.869210
146.345531	5387.488764	24.874227
146.272869	5397.726925	24.879245
146.427192	5394.391206	24.884263
146.269115	5393.836205	24.889280
146.552462	5402.374880	24.894298
146.715969	5410.327743	24.899315
146.676164	5418.793912	24.904333
147.048021	5414.295132	24.909351
147.030393	5444.350241	24.914368
147.088588	5444.859698	24.919386
147.312449	5445.591396	24.924403
147.321432	5463.719571	24.929421
147.684369	5469.227837	24.934439
147.694966	5475.660003	24.939456
147.969506	5483.029028	24.944474
147.804145	5508.662749	24.949491
147.946825	5512.922141	24.954509
148.686401	5523.446487	24.959527
148.599114	5531.596088	24.964544
148.955572	5533.206848	24.969562
148.935640	5535.807710	24.974579
148.831794	5538.420891	24.979597
149.582802	5558.268516	24.984615
149.434165	5568.130291	24.989632
149.429172	5566.919074	24.994650
149.632512	5577.531447	24.999667
149.795547	5590.351051	25.004685
150.229775	5591.217262	25.009703
150.307119	5590.311389	25.014720
150.421690	5591.064338	25.019738
150.424755	5597.422191	25.024755
150.362024	5616.218484	25.029773
150.904605	5622.319267	25.034791
150.857958	5627.911938	25.039808
150.867478	5633.422853	25.044826
151.025811	5650.020622	25.049843
151.391270	5653.475257	25.054861
151.215560	5645.652022	25.059879
151.755047	5678.458585	25.064896
151.988542	5683.903296	25.069914
152.616439	5683.571796	25.074931
152.281713	5688.733318	25.079949
152.589600	5678.289981	25.084967
152.308383	5688.674697	25.089984
152.170229	5677.864146	25.095002
152.502810	5690.461225	25.100019
152.335516	5703.862517	25.105037
152.704711	5704.533150	25.110055
152.540976	5724.504072	25.115072
152.987865	5734.750949	25.120090
153.380778	5740.323658	25.125107
153.244300	5767.808619	25.130125
153.813717	5756.552439	25.135143
154.002144	5770.467487	25.140160
153.630243	5778.032672	25.145178
154.251247	5780.180129	25.150195
154.313871	5802.376475	25.155213
154.459882	5788.199029	25.160231
154.391951	5808.969373	25.165248
154.452373	5821.900667	25.170266
154.977466	5820.062946	25.175283
155.260526	5829.217812	25.180301
155.674359	5844.895301	25.185319
155.328543	5855.364855	25.190336
155.712267	5850.303209	25.195354
155.649428	5852.510333	25.200371
155.648157	5859.537691	25.205389
156.561800	5874.848135	25.210407
156.498907	5874.743625	25.215424
156.487196	5879.722564	25.220442
156.693136	5876.359296	25.225459
156.294806	5890.940248	25.230477
156.806053	5895.414390	25.235495
156.994516	5907.525128	25.240512
157.069457	5913.774332	25.245530
157.439854	5924.123784	25.250547
157.424842	5944.791819	25.255565
157.358477	5945.801573	25.260583
157.781142	5950.179343	25.265600
157.738085	5965.802635	25.270618
158.152491	5966.901347	25.275635
157.813410	5968.913996	25.280653
158.675309	5981.924603	25.285671
158.821975	5992.441884	25.290688
158.715239	5990.490576	25.295706
159.115865	5990.459763	25.300723
159.023012	6009.107924	25.305741
159.328408	6013.624056	25.310759
159.462879	6024.115023	25.315776
159.412157	6021.680290	25.320794
160.015079	6039.132682	25.325811
159.818519	6056.346481	25.330829
160.257620	6048.911949	25.335847
160.437428	6054.520051	25.340864
160.047972	6058.195058	25.345882
160.657401	6065.950771	25.350899
160.310793	6076.808113	25.355917
160.887716	6081.494333	25.360935
160.876391	6088.599858	25.365952
161.519986	6100.907126	25.370970
161.396054	6105.224994	25.375987
161.687033	6109.736452	25.381005
161.957520	6112.435040	25.386023
161.813482	6121.693865	25.391040
161.636516	6141.759655	25.396058
162.463251	6135.814897	25.401075
162.208551	6148.750584	25.406093
162.310142	6152.750733	25.411111
162.447309	6164.106162	25.416128
162.560430	6160.687314	25.421146
162.915469	6169.760364	25.426163
162.875376	6188.867853	25.431181
163.212274	6192.564413	25.436199
163.265713	6193.907995	25.441216
162.957441	6190.222586	25.446234
163.449637	6203.810481	25.451251
163.558280	6214.835926	25.456269
163.752578	6229.921613	25.461287
164.017379	6246.186543	25.466304
164.046428	6251.143885	25.471322
164.334845	6248.378087	25.476339
164.414502	6266.150499	25.481357
164.822515	6277.600581	25.486375
164.867137	6283.051564	25.491392
164.482100	6302.987390	25.496410
165.016434	6304.423859	25.501427
165.629319	6320.851777	25.506445
165.385364	6330.102848	25.511463
165.748890	6337.013316	25.516480
165.786648	6347.121177	25.521498
166.289278	6355.602801	25.526515
166.238263	6367.009221	25.531533
166.459316	6366.130709	25.536551
166.763453	6378.318750	25.541568
166.685457	6399.017496	25.546586
166.966477	6384.333555	25.551603
167.165484	6407.607715	25.556621
167.484165	6417.862086	25.561639
168.118146	6419.567984	25.566656
167.783154	6421.575285	25.571674
167.883291	6420.925514	25.576691
168.082856	6428.996581	25.581709
168.030650	6443.801924	25.586727
168.157785	6446.914973	25.591744
168.423314	6461.288875	25.596762
168.723619	6465.887108	25.601779
168.950670	6476.186617	25.606797
169.138894	6475.759341	25.611815
169.526089	6482.077585	25.616832
169.389519	6499.474117	25.621850
169.761480	6500.956391	25.626867
169.547202	6511.496754	25.631885
169.543746	6517.845816	25.636903
170.209646	6526.083113	25.641920
170.216421	6530.968616	25.646938
170.494454	6537.570391	25.651955
170.491875	6548.015870	25.656973
170.651221	6557.364924	25.661991
171.206000	6558.326233	25.667008
171.043946	6567.270878	25.672026
171.333332	6581.559812	25.677044
171.514623	6589.248039	25.682061
171.401642	6588.291703	25.687079
172.041672	6594.257014	25.692096
172.321652	6609.558872	25.697114
172.087962	6612.813604	25.702132
172.149898	6610.062398	25.707149
172.530864	6618.331162	25.712167
172.739806	6634.060684	25.717184
173.163866	6641.648097	25.722202
173.237720	6647.800890	25.727220
173.264108	6640.041372	25.732237
173.020772	6650.890671	25.737255
173.616929	6673.244871	25.742272
173.632150	6678.098303	25.747290
173.767497	6665.583787	25.752308
173.727970	6698.029125	25.757325
173.839158	6714.302639	25.762343
174.038405	6714.570607	25.767360
174.136971	6732.738964	25.772378
174.692493	6737.217836	25.777396
174.714883	6742.856182	25.782413
175.003466	6757.414786	25.787431
175.324614	6765.549390	25.792448
175.050425	6773.524203	25.797466
175.136835	6774.533923	25.802484
175.352064	6790.474440	25.807501
175.665278	6791.806573	25.812519
175.977205	6799.396085	25.817536
176.224813	6834.881004	25.822554
176.367839	6834.825102	25.827572
176.705152	6839.848956	25.832589
176.869492	6855.521494	25.837607
176.837265	6850.740276	25.842624
176.971662	6864.557322	25.847642
177.006343	6872.312492	25.852660
177.345747	6883.584547	25.857677
177.507936	6887.359030	25.862695
177.910240	6895.543278	25.867712
177.981871	6917.352165	25.872730
178.338228	6923.520522	25.877748
178.199371	6925.386716	25.882765
178.404267	6947.577655	25.887783
178.619485	6949.342701	25.892800
178.530710	6962.116099	25.897818
179.479123	6970.407683	25.902836
179.557510	6977.673616	25.907853
179.342550	6983.486031	25.912871
179.616091	6975.539715	25.917888
179.852923	7003.588848	25.922906
179.860292	7010.767306	25.927924
180.108643	7010.196159	25.932941
180.315947	7027.783669	25.937959
180.318719	7028.526053	25.942976
180.547385	7046.774054	25.947994
180.980425	7062.803238	25.953012
180.859003	7066.329339	25.958029
180.740766	7083.217789	25.963047
181.366343	7077.313080	25.968064
181.549329	7086.916890	25.973082
181.412990	7100.759270	25.978100
181.933297	7114.438606	25.983117
181.501475	7128.621367	25.988135
182.403990	7135.802925	25.993152
182.460636	7150.484570	25.998170
182.764158	7162.214102	26.003188
183.098728	7171.892904	26.008205
183.036761	7179.304255	26.013223
183.318217	7185.858474	26.018240
183.610393	7207.123194	26.023258
183.695206	7215.824112	26.028276
184.202112	7215.515775	26.033293
183.899441	7217.484740	26.038311
184.238176	7226.439795	26.043328
184.095842	7242.820410	26.048346
184.423707	7241.442898	26.053364
184.881384	7257.973105	26.058381
184.534102	7267.701043	26.063399
185.204775	7268.637701	26.068416
184.886215	7289.093076	26.073434
185.276601	7311.692555	26.078452
185.459357	7310.164981	26.083469
185.564224	7330.283286	26.088487
185.944342	7328.396148	26.093504
186.048419	7347.161362	26.098522
186.755011	7364.045103	26.103540
186.438493	7356.034018	26.108557
186.431722	7365.969519	26.113575
186.859227	7372.062472	26.118592
187.190327	7391.797607	26.123610
187.123449	7398.990108	26.128628
187.596997	7398.504547	26.133645
187.673249	7420.978957	26.138663
187.719159	7424.009547	26.143680
188.223100	7428.053688	26.148698
188.010180	7439.372676	26.153716
188.526752	7453.798080	26.158733
188.534867	7455.061052	26.163751
188.751520	7454.351778	26.168768
188.756166	7468.688651	26.173786
189.031171	7483.595181	26.178804
189.162570	7494.631927	26.183821
189.409386	7512.522209	26.188839
189.839596	7505.272798	26.193856
189.995339	7517.398062	26.198874
190.100605	7533.248039	26.203892
190.261241	7533.652386	26.208909
190.140787	7547.987197	26.213927
190.785331	7560.466383	26.218944
190.937559	7569.142943	26.223962
190.772498	7573.999712	26.228980
191.240503	7584.799626	26.233997
191.308846	7604.899119	26.239015
191.511983	7605.528802	26.244032
192.118514	7626.948422	26.249050
191.634813	7627.313713	26.254068
192.143172	7636.648949	26.259085
191.991805	7659.685986	26.264103
192.406697	7669.432928	26.269120
193.071791	7683.977317	26.274138
192.758817	7697.543039	26.279156
193.263960	7698.193624	26.284173
193.485460	7718.071766	26.289191
193.712442	7721.508038	26.294208
193.698536	7730.448501	26.299226
194.038971	7741.326356	26.304244
194.400724	7745.276750	26.309261
194.439436	7751.078170	26.314279
194.634252	7754.908114	26.319296
194.527216	7778.904499	26.324314
194.847448	7781.464382	26.329332
195.306116	7790.314043	26.334349
195.122743	7810.943057	26.339367
195.546112	7811.527626	26.344384
195.935259	7825.194631	26.349402
195.712231	7841.443492	26.354420
196.016684	7836.961500	26.359437
195.773039	7858.919182	26.364455
196.263668	7869.129487	26.369472
196.680089	7886.788095	26.374490
196.837511	7905.634148	26.379508
197.244416	7894.951624	26.384525
197.263369	7913.780435	26.389543
197.495244	7928.479477	26.394560
197.441944	7926.263074	26.399578
197.850688	7947.898620	26.404596
198.205742	7960.893950	26.409613
198.286309	7966.786196	26.414631
198.431081	7981.984152	26.419648
199.038002	7984.343004	26.424666
199.201487	7987.463730	26.429684
199.390893	7989.765666	26.434701
199.714735	7996.603086	26.439719
199.670872	8015.987518	26.444736
199.770294	8017.406354	26.449754
199.718335	8030.548679	26.454772
200.266777	8027.377183	26.459789
199.851515	8040.651342	26.464807
200.457748	8039.592397	26.469824
200.779966	8045.064199	26.474842
200.244569	8067.554126	26.479860
200.995138	8066.246784	26.484877
200.955173	8078.608894	26.489895
201.155060	8102.210721	26.494912
201.310628	8107.436792	26.499930
201.233781	8137.705305	26.504948
201.520810	8141.127790	26.509965
201.674674	8158.830165	26.514983
202.025492	8179.053768	26.520000
202.505840	8185.083935	26.525018
202.406574	8203.842858	26.530036
202.897562	8215.613031	26.535053
203.244422	8238.487287	26.540071
203.210083	8233.228638	26.545088
203.702815	8252.094426	26.550106
203.679487	8276.904819	26.555124
204.133886	8271.197380	26.560141
204.230782	8295.275790	26.565159
204.759607	8300.308583	26.570176
204.854100	8293.243583	26.575194
204.599695	8317.763808	26.580212
204.974849	8323.783084	26.585229
205.567202	8323.997037	26.590247
205.400375	8342.836627	26.595264
205.626941	8351.075931	26.600282
205.844475	8369.172108	26.605300
206.007204	8386.214720	26.610317
206.368632	8386.548038	26.615335
206.526615	8406.313092	26.620352
207.024096	8409.700796	26.625370
207.342737	8417.580650	26.630388
207.221716	8412.492265	26.635405
207.769117	8423.701049	26.640423
207.732414	8448.988931	26.645440
207.903910	8444.772980	26.650458
207.870619	8461.380992	26.655476
208.066376	8470.989826	26.660493
208.134628	8485.176076	26.665511
208.267730	8507.538623	26.670528
209.034334	8510.714009	26.675546
209.010322	8519.965382	26.680564
208.977471	8542.608316	26.685581
209.058277	8557.562180	26.690599
208.916380	8562.559569	26.695616
210.052561	8578.634587	26.700634
209.979311	8603.446661	26.705652
209.979613	8603.304097	26.710669
210.327882	8622.949690	26.715687
210.309499	8639.628680	26.720704
211.059545	8646.843268	26.725722
211.019034	8670.560567	26.730740
211.164632	8678.302980	26.735757
211.535168	8685.437040	26.740775
211.560350	8695.469699	26.745792
211.952712	8711.025178	26.750810
212.077772	8725.790690	26.755828
212.276245	8722.513931	26.760845
212.488355	8745.811400	26.765863
212.769177	8758.828336	26.770880
213.104488	8769.870810	26.775898
213.330514	8786.606386	26.780916
213.122293	8784.694376	26.785933
213.376130	8809.557394	26.790951
213.697604	8814.600257	26.795968
213.971137	8833.079206	26.800986
214.034350	8850.915519	26.806004
214.316393	8844.852771	26.811021
214.551301	8860.898453	26.816039
215.020827	8870.774161	26.821056
215.162618	8878.862342	26.826074
215.219895	8895.800063	26.831092
215.466424	8901.420974	26.836109
215.780754	8908.676302	26.841127
215.848615	8920.270473	26.846144
215.988618	8938.250148	26.851162
216.220535	8950.055089	26.856180
216.540132	8954.598864	26.861197
216.754802	8967.481972	26.866215
216.775261	8995.204116	26.871232
217.370163	8994.332118	26.876250
217.595210	9011.442281	26.881268
217.560874	9020.696440	26.886285
218.044052	9027.453572	26.891303
218.216809	9047.833008	26.896320
217.906233	9056.416833	26.901338
218.371327	9070.788420	26.906356
218.612475	9082.654952	26.911373
219.112251	9098.738954	26.916391
219.047522	9121.009063	26.921408
219.503258	9120.680027	26.926426
219.329297	9143.766264	26.931444
219.595070	9155.186044	26.936461
219.899808	9172.520308	26.941479
220.329980	9185.394702	26.946496
220.471713	9194.856148	26.951514
220.382741	9220.663591	26.956532
221.019769	9229.870543	26.961549
221.345712	9244.920754	26.966567
221.256988	9262.214686	26.971584
221.659230	9262.516850	26.976602
221.568996	9283.694028	26.981620
221.991821	9299.090633	26.986637
222.116100	9313.934019	26.991655
222.472325	9333.215212	26.996672
222.896922	9342.099741	27.001690
222.671415	9361.254325	27.006708
223.042498	9376.856516	27.011725
223.322027	9381.965588	27.016743
223.749183	9405.649096	27.021760
224.097091	9409.768425	27.026778
223.958736	9430.126584	27.031796
224.280216	9442.531537	27.036813
224.599731	9461.426643	27.041831
224.832207	9478.148482	27.046848
225.049423	9480.488573	27.051866
224.964801	9511.353385	27.056884
225.509939	9513.473760	27.061901
225.894029	9520.549231	27.066919
225.740012	9539.578750	27.071936
226.329935	9543.428803	27.076954
226.742459	9557.853648	27.081972
226.665083	9562.258486	27.086989
227.011559	9567.918233	27.092007
227.005525	9582.324155	27.097024
227.346372	9590.290723	27.102042
227.611370	9614.715916	27.107060
227.590281	9618.576536	27.112077
227.916014	9633.486920	27.117095
228.215509	9651.128237	27.122112
228.251923	9658.509479	27.127130
228.555141	9678.170917	27.132148
228.477052	9693.549195	27.137165
229.143964	9688.166108	27.142183
229.137056	9716.343862	27.147200
229.391523	9725.928764	27.152218
229.477236	9739.687820	27.157236
229.781706	9756.657220	27.162253
230.167393	9764.039779	27.167271
230.263552	9787.347715	27.172288
230.570430	9783.914143	27.177306
230.650308	9801.249284	27.182324
230.934925	9815.426893	27.187341
230.984631	9833.470575	27.192359
231.456810	9866.370980	27.197376
231.302458	9873.293882	27.202394
231.871567	9888.919727	27.207412
232.211853	9908.443746	27.212429
232.513451	9912.058006	27.217447
232.657088	9924.236733	27.222464
232.664226	9935.921259	27.227482
233.032247	9953.802878	27.232500
233.182809	9975.758069	27.237517
233.604623	9989.539696	27.242535
233.582281	10019.397796	27.247552
234.463949	10011.996904	27.252570
234.450323	10027.690986	27.257588
234.489019	10043.908201	27.262605
234.963970	10056.981506	27.267623
234.933034	10062.355689	27.272640
235.320223	10076.420435	27.277658
235.516256	10097.630078	27.282676
235.570560	10100.730691	27.287693
236.073105	10125.786199	27.292711
236.237629	10138.560377	27.297728
236.510525	10154.552220	27.302746
236.928069	10160.933092	27.307764
236.529850	10175.058609	27.312781
236.806375	10188.426426	27.317799
237.159312	10207.153010	27.322816
237.543719	10221.928177	27.327834
237.726324	10239.388593	27.332852
237.811911	10263.240994	27.337869
238.384636	10275.816930	27.342887
238.688068	10289.756282	27.347904
238.550855	10312.038461	27.352922
239.217775	10324.899006	27.357940
239.307212	10350.101244	27.362957
239.588865	10355.864967	27.367975
239.750560	10376.763164	27.372992
240.020432	10383.300926	27.378010
240.603653	10398.818575	27.383028
240.556269	10415.386819	27.388045
240.910861	10419.966978	27.393063
241.266577	10449.659298	27.398080
241.311152	10453.937833	27.403098
241.773267	10469.414147	27.408116
241.767175	10482.310593	27.413133
242.127178	10488.273324	27.418151
242.394587	10509.242432	27.423168
242.286954	10525.325209	27.428186
242.916404	10534.013409	27.433204
242.921432	10548.735863	27.438221
243.411165	10562.752548	27.443239
243.458412	10575.274679	27.448256
243.683292	10585.990036	27.453274
244.142819	10601.247096	27.458292
244.532213	10613.759892	27.463309
244.767625	10631.822574	27.468327
244.614751	10645.745591	27.473344
244.911706	10643.501558	27.478362
245.242982	10656.449445	27.483380
245.086639	10672.914661	27.488397
245.350983	10681.297816	27.493415
245.578120	10712.060533	27.498432
245.961426	10723.109018	27.503450
246.537521	10736.526972	27.508468
246.314645	10756.436749	27.513485
246.957533	10765.378116	27.518503
247.084448	10780.726646	27.523520
247.095094	10787.576143	27.528538
247.356718	10800.724761	27.533556
247.474178	10822.738584	27.538573
247.781066	10836.097187	27.543591
247.990966	10859.304333	27.548608
248.343284	10872.143337	27.553626
248.832854	10890.901675	27.558644
248.807736	10907.088564	27.563661
249.282059	10924.689733	27.568679
249.465730	10938.801530	27.573696
249.519763	10960.195750	27.578714
250.214551	10972.559001	27.583732
249.970083	10999.640643	27.588749
250.345579	11003.064074	27.593767
250.797298	11027.786680	27.598784
250.791745	11038.431757	27.603802
251.102333	11050.981574	27.608820
251.140643	11081.037230	27.613837
251.702299	11089.226416	27.618855
251.823068	11103.041499	27.623872
252.205915	11130.288971	27.628890
252.699858	11144.354315	27.633908
252.718072	11158.411753	27.638925
253.342187	11177.160759	27.643943
253.377612	11186.369946	27.648960
253.750342	11201.339400	27.653978
253.795766	11213.914327	27.658996
254.144882	11238.966240	27.664013
254.647017	11249.246933	27.669031
254.793704	11262.421257	27.674048
254.934851	11275.371175	27.679066
255.367382	11289.921115	27.684084
255.623080	11308.077318	27.689101
255.933570	11309.776663	27.694119
256.050550	11327.900699	27.699136
255.880880	11347.783485	27.704154
256.626595	11361.077763	27.709172
256.569996	11381.706122	27.714189
257.017642	11398.102034	27.719207
257.547848	11404.651484	27.724224
257.596679	11416.215936	27.729242
258.054796	11438.139541	27.734260
257.888169	11445.108479	27.739277
258.393361	11462.906827	27.744295
258.375184	11474.641566	27.749312
258.963647	11495.086078	27.754330
259.589763	11500.303915	27.759348
259.360732	11515.626971	27.764365
259.536879	11535.251044	27.769383
260.099158	11533.122127	27.774400
260.212340	11553.812420	27.779418
260.429647	11561.352897	27.784436
260.679534	11587.050514	27.789453
260.997283	11598.994469	27.794471
261.121549	11612.948079	27.799488
260.887017	11637.563028	27.804506
261.570978	11645.971775	27.809524
261.440654	11670.240183	27.814541
261.957712	11688.911383	27.819559
262.208962	11696.903286	27.824576
262.500683	11722.909353	27.829594
262.977906	11728.356766	27.834612
262.727063	11738.253428	27.839629
263.320556	11757.964693	27.844647
263.544400	11779.390191	27.849664
263.902386	11795.185208	27.854682
264.181259	11798.202489	27.859700
264.537641	11816.589999	27.864717
264.694703	11825.073451	27.869735
264.803269	11847.974172	27.874752
264.978935	11859.076717	27.879770
265.371416	11878.481026	27.884788
265.894286	11891.557350	27.889805
266.123610	11919.690386	27.894823
266.162897	11935.185310	27.899840
266.490219	11945.571025	27.904858
266.958047	11956.332173	27.909876
266.892626	11982.660938	27.914893
267.485024	11989.846423	27.919911
267.770620	12009.664115	27.924928
267.976800	12028.812641	27.929946
268.392035	12039.450180	27.934964
268.574724	12057.477485	27.939981
268.660313	12068.744788	27.944999
268.803108	12084.484310	27.950016
269.129705	12103.798942	27.955034
269.538295	12117.007825	27.960052
269.679697	12133.422085	27.965069
269.985637	12149.079510	27.970087
270.238576	12174.484446	27.975104
270.356375	12187.393260	27.980122
270.610333	12198.327069	27.985140
270.905888	12217.908566	27.990157
271.403474	12244.579496	27.995175
271.821962	12258.603149	28.000192
271.957990	12277.735216	28.005210
272.406525	12299.552842	28.010228
272.263562	12316.142001	28.015245
272.717059	12334.592817	28.020263
273.438388	12347.438102	28.025280
273.431584	12370.353929	28.030298
273.929303	12377.519015	28.035316
273.747440	12407.868865	28.040333
274.078610	12430.806051	28.045351
274.583852	12443.975565	28.050368
274.607974	12455.792260	28.055386
275.057146	12464.364796	28.060404
275.024676	12494.401693	28.065421
275.237639	12513.184065	28.070439
275.808215	12534.163925	28.075456
276.083226	12563.655227	28.080474
276.275043	12580.477627	28.085492
276.558995	12593.710682	28.090509
276.740271	12603.356690	28.095527
277.093081	12620.335285	28.100544
277.658164	12646.135268	28.105562
277.900648	12661.061447	28.110580
278.121552	12669.254265	28.115597
278.233981	12700.046048	28.120615
279.013520	12711.734736	28.125632
279.076420	12728.014456	28.130650
279.368491	12737.254533	28.135668
279.696549	12762.050688	28.140685
279.818801	12769.500301	28.145703
280.153947	12773.821179	28.150720
279.992893	12798.015983	28.155738
280.568756	12816.757548	28.160756
280.817279	12838.344254	28.165773
280.876151	12850.032561	28.170791
281.252573	12864.613695	28.175808
281.335829	12879.744509	28.180826
281.779037	12890.516659	28.185844
281.868934	12912.350348	28.190861
282.142528	12932.032472	28.195879
282.971227	12948.606424	28.200896
282.814724	12969.573244	28.205914
283.102027	12987.803318	28.210932
283.556022	13004.907400	28.215949
283.912134	13021.216100	28.220967
283.816991	13030.309263	28.225984
283.979761	13062.101992	28.231002
284.627279	13079.257644	28.236020
284.984988	13092.989500	28.241037
285.232799	13119.975850	28.246055
285.392529	13134.824757	28.251072
285.480157	13152.115712	28.256090
285.994665	13172.692783	28.261108
286.241499	13187.114423	28.266125
286.473083	13220.809266	28.271143
286.629485	13243.735553	28.276160
286.820962	13268.435315	28.281178
287.350671	13282.271242	28.286196
287.610779	13304.840043	28.291213
287.893725	13324.417080	28.296231
288.436609	13350.863272	28.301248
288.694555	13361.065960	28.306266
289.155158	13382.870437	28.311284
289.571681	13412.713357	28.316301
289.842046	13424.217352	28.321319
290.340685	13445.071613	28.326336
290.110093	13466.848774	28.331354
290.420572	13473.931872	28.336372
290.591087	13495.277053	28.341389
291.134105	13509.241776	28.346407
291.119788	13525.022881	28.351424
291.569269	13554.428787	28.356442
292.023502	13583.023905	28.361460
292.312671	13589.670883	28.366477
292.851663	13626.826971	28.371495
293.469864	13626.192031	28.376512
293.638869	13640.251870	28.381530
294.005530	13642.046186	28.386548
294.191762	13663.532401	28.391565
293.944907	13675.457871	28.396583
294.578769	13684.947656	28.401600
294.919893	13709.791948	28.406618
294.587002	13720.521328	28.411636
295.461796	13739.832270	28.416653
295.687922	13756.275118	28.421671
295.944133	13767.687139	28.426688
296.252481	13798.610895	28.431706
296.654740	13806.507924	28.436724
296.633912	13835.826704	28.441741
296.981141	13844.881769	28.446759
297.352687	13869.781157	28.451776
297.517134	13886.442379	28.456794
297.461418	13910.347166	28.461812
297.916987	13929.278559	28.466829
298.059912	13956.037794	28.471847
298.412381	13984.139829	28.476864
298.531698	14008.353056	28.481882
299.347861	14034.625891	28.486900
299.884477	14044.923148	28.491917
299.669420	14069.169746	28.496935
300.355844	14086.545396	28.501952
300.712704	14100.818823	28.506970
300.703395	14119.230068	28.511988
301.208767	14128.976211	28.517005
301.505813	14151.653543	28.522023
301.434681	14153.411635	28.527040
302.077684	14175.119212	28.532058
302.345072	14203.459505	28.537076
302.673666	14205.963101	28.542093
302.898914	14228.222164	28.547111
303.069943	14243.221510	28.552128
303.457487	14265.136975	28.557146
303.593503	14287.045244	28.562164
303.879165	14295.046918	28.567181
304.337632	14328.135960	28.572199
304.846705	14342.828852	28.577216
304.740732	14371.986165	28.582234
305.063074	14393.550101	28.587252
305.334266	14418.050855	28.592269
305.430910	14444.850069	28.597287
306.358593	14461.552609	28.602304
306.543573	14489.268730	28.607322
307.060890	14510.961308	28.612340
307.182491	14536.831388	28.617357
307.606272	14554.153293	28.622375
307.830580	14565.713000	28.627392
308.084417	14582.508286	28.632410
308.340667	14613.369704	28.637428
308.660031	14627.799525	28.642445
308.800971	14651.356049	28.647463
309.356273	14673.783315	28.652480
309.708537	14687.865733	28.657498
310.137767	14717.379531	28.662516
310.684769	14728.439907	28.667533
310.866100	14749.078844	28.672551
311.207950	14775.749752	28.677568
310.930707	14784.024511	28.682586
311.624732	14806.083832	28.687604
311.932102	14813.149116	28.692621
312.178090	14843.282931	28.697639
312.240873	14866.308944	28.702656
312.797878	14886.813373	28.707674
312.805728	14909.883213	28.712692
313.477917	14933.743086	28.717709
313.897262	14958.609426	28.722727
314.340787	14973.985159	28.727744
314.489218	14997.695399	28.732762
314.685883	15007.562515	28.737780
315.097418	15028.300823	28.742797
315.433635	15048.990154	28.747815
315.777623	15064.774903	28.752832
316.198382	15091.658649	28.757850
316.716811	15110.116050	28.762868
316.885613	15117.335220	28.767885
317.197005	15144.349060	28.772903
317.181735	15170.036318	28.777920
317.823254	15182.750486	28.782938
317.877488	15202.446434	28.787956
318.212463	15214.489493	28.792973
318.328696	15238.288945	28.797991
318.996573	15259.295616	28.803008
319.184322	15277.569941	28.808026
319.607483	15304.820880	28.813044
320.105512	15315.241965	28.818061
320.467191	15337.768387	28.823079
320.751754	15349.395906	28.828096
320.683748	15365.567518	28.833114
320.992808	15391.494605	28.838132
321.493429	15399.272102	28.843149
321.507398	15422.174575	28.848167
321.815799	15435.850367	28.853184
322.115921	15464.943978	28.858202
322.245370	15489.643170	28.863220
322.563913	15509.510097	28.868237
322.833477	15532.531187	28.873255
323.038606	15549.709077	28.878272
323.372429	15579.801333	28.883290
323.779820	15617.231178	28.888308
324.422789	15627.787667	28.893325
324.195397	15658.062797	28.898343
324.880510	15684.129853	28.903360
325.269000	15702.458115	28.908378
324.920470	15745.413378	28.913396
325.786565	15758.511666	28.918413
326.145338	15790.092829	28.923431
326.325590	15805.047941	28.928448
327.067053	15843.956646	28.933466
327.038787	15870.810380	28.938484
327.735337	15900.966131	28.943501
328.073755	15915.486927	28.948519
328.606226	15946.260995	28.953536
328.957452	15962.937543	28.958554
329.075533	15981.555185	28.963572
329.716126	16005.803291	28.968589
329.824692	16020.633334	28.973607
330.163311	16051.944072	28.978624
330.797638	16068.926944	28.983642
330.587600	16090.940604	28.988660
331.303799	16108.753245	28.993677
331.723976	16122.370126	28.998695
332.234353	16149.748314	29.003712
332.343523	16158.078018	29.008730
332.420513	16181.789176	29.013748
332.746218	16205.208582	29.018765
332.532757	16232.725626	29.023783
332.979620	16261.645037	29.028800
334.011931	16282.783425	29.033818
334.018893	16313.430788	29.038836
334.495880	16329.292466	29.043853
335.005783	16357.563232	29.048871
335.079700	16365.172225	29.053888
335.434026	16400.169447	29.058906
335.819122	16425.754563	29.063924
336.451066	16434.243777	29.068941
336.644406	16468.353560	29.073959
336.725418	16483.577914	29.078976
337.599429	16504.898839	29.083994
337.365326	16537.013032	29.089012
337.917759	16550.843242	29.094029
338.519329	16576.142136	29.099047
338.439560	16603.257787	29.104064
338.986204	16618.039502	29.109082
339.117758	16641.486932	29.114100
339.825305	16661.765323	29.119117
339.980123	16690.528906	29.124135
340.329704	16710.853994	29.129152
340.642628	16720.765947	29.134170
340.560985	16763.974442	29.139188
341.177317	16783.850364	29.144205
341.509679	16808.549469	29.149223
341.788338	16823.429318	29.154240
342.399323	16854.606650	29.159258
342.571690	16874.991221	29.164276
342.689418	16894.158499	29.169293
343.345152	16916.628953	29.174311
343.471649	16951.578352	29.179328
343.923011	16956.800099	29.184346
344.070699	16987.589352	29.189364
344.633341	17009.621364	29.194381
345.202575	17025.181556	29.199399
345.442977	17050.444799	29.204416
346.018678	17051.899101	29.209434
345.901832	17084.563994	29.214452
346.216528	17098.353620	29.219469
346.487631	17120.862791	29.224487
346.744599	17151.533378	29.229504
346.959542	17171.137291	29.234522
347.174911	17209.259853	29.239540
347.935041	17224.662532	29.244557
348.093257	17254.039723	29.249575
348.224388	17285.486447	29.254592
348.712515	17306.252779	29.259610
348.838435	17348.630814	29.264628
349.346877	17368.484313	29.269645
350.119615	17399.137776	29.274663
350.256092	17430.951180	29.279680
350.873694	17458.540784	29.284698
351.146017	17483.365907	29.289716
351.412881	17505.761228	29.294733
351.981853	17524.789920	29.299751
351.990713	17549.851063	29.304768
352.786477	17573.583968	29.309786
352.829761	17597.274355	29.314804
352.963746	17624.085159	29.319821
353.347097	17655.572810	29.324839
353.678401	17679.679098	29.329856
354.544458	17706.641584	29.334874
354.637042	17749.067142	29.339892
355.166867	17764.500562	29.344909
355.631077	17796.460624	29.349927
355.844596	17812.810298	29.354944
356.284641	17830.919578	29.359962
356.810955	17865.574575	29.364980
357.103859	17882.710409	29.369997
357.699322	17904.752369	29.375015
357.571407	17929.422128	29.380032
357.660468	17944.288648	29.385050
358.168967	17983.103801	29.390068
358.626540	18006.927982	29.395085
359.352621	18022.092700	29.400103
359.369201	18055.263934	29.405120
359.945941	18071.348814	29.410138
360.152874	18111.900937	29.415156
360.370290	18139.605200	29.420173
361.071786	18152.262876	29.425191
361.219759	18187.279104	29.430208
361.618179	18200.917066	29.435226
361.951475	18236.085590	29.440244
362.182680	18269.095612	29.445261
362.916420	18284.979732	29.450279
363.067255	18321.890639	29.455296
363.335895	18339.549606	29.460314
364.025467	18370.453519	29.465332
364.213994	18398.812488	29.470349
364.528639	18418.484923	29.475367
364.634109	18454.815618	29.480384
365.558276	18466.016303	29.485402
365.889723	18500.004931	29.490420
365.926942	18515.484321	29.495437
366.531924	18539.445667	29.500455
366.558522	18567.822264	29.505472
366.794284	18580.521090	29.510490
367.431208	18624.931829	29.515508
367.271755	18644.826455	29.520525
368.007359	18670.538317	29.525543
368.365361	18699.760452	29.530560
368.866287	18714.644623	29.535578
369.424550	18745.998189	29.540596
369.466206	18758.588971	29.545613
369.523002	18784.976156	29.550631
369.984072	18808.182928	29.555648
370.519559	18842.584628	29.560666
370.737113	18871.060983	29.565684
371.157000	18891.342424	29.570701
371.576818	18922.750765	29.575719
371.744084	18950.114694	29.580736
372.254562	18967.792633	29.585754
372.697039	18998.735455	29.590772
372.848269	19038.258558	29.595789
373.718688	19054.934271	29.600807
373.759123	19093.976092	29.605824
374.168478	19119.364281	29.610842
374.805000	19137.595389	29.615860
375.165942	19181.235076	29.620877
375.714291	19188.349066	29.625895
375.822510	19219.089067	29.630912
376.484957	19248.205021	29.635930
376.680145	19266.495124	29.640948
376.889929	19302.764678	29.645965
377.298703	19327.448572	29.650983
377.677080	19367.521329	29.656000
377.763978	19392.392595	29.661018
378.350819	19423.462082	29.666036
378.681637	19457.648252	29.671053
379.319368	19480.943386	29.676071
379.120637	19521.837233	29.681088
379.853260	19549.753382	29.686106
380.325418	19587.033263	29.691124
379.973757	19614.283937	29.696141
381.076011	19638.840908	29.701159
381.298926	19683.816443	29.706176
381.677677	19705.128869	29.711194
382.604673	19734.711117	29.716212
382.527375	19778.825337	29.721229
382.864250	19794.902711	29.726247
383.348720	19836.384251	29.731264
383.639616	19870.372915	29.736282
384.422655	19898.287609	29.741300
384.258792	19933.467884	29.746317
384.859627	19960.304497	29.751335
385.053047	20000.458250	29.756352
385.989149	20029.531852	29.761370
386.512171	20060.540560	29.766388
386.693671	20081.857731	29.771405
387.343419	20112.232264	29.776423
387.132840	20148.700921	29.781440
387.885487	20165.662110	29.786458
388.609890	20195.709118	29.791476
388.288818	20225.309597	29.796493
389.196914	20246.525645	29.801511
389.352088	20275.628014	29.806528
389.644647	20309.510082	29.811546
390.342199	20337.281995	29.816564
390.237814	20372.431270	29.821581
390.552171	20395.335010	29.826599
391.209596	20423.686023	29.831616
391.492583	20470.000163	29.836634
392.157685	20496.311439	29.841652
392.378233	20535.793486	29.846669
392.431263	20552.407321	29.851687
392.914464	20594.259878	29.856704
393.488804	20622.949767	29.861722
393.800053	20646.896530	29.866740
394.045850	20681.993225	29.871757
394.307306	20706.944760	29.876775
394.673890	20736.832801	29.881792
395.327875	20754.127825	29.886810
395.731455	20781.003126	29.891828
396.025593	20823.535552	29.896845
396.568154	20847.833756	29.901863
396.757299	20882.985970	29.906880
396.785661	20913.653992	29.911898
397.245689	20952.618073	29.916916
397.659475	20986.722672	29.921933
398.059265	21020.627842	29.926951
398.773774	21069.090611	29.931968
398.572387	21112.700666	29.936986
399.393317	21140.666342	29.942004
399.883475	21178.402440	29.947021
400.327749	21212.492991	29.952039
400.599086	21239.740938	29.957056
400.944901	21284.665722	29.962074
401.504421	21312.370642	29.967092
401.778412	21351.896209	29.972109
402.577685	21388.897325	29.977127
403.122587	21426.617035	29.982144
403.101348	21452.562493	29.987162
403.817291	21485.148585	29.992180
404.057759	21525.627722	29.997197
404.419248	21563.272450	30.002215
404.929165	21600.489052	30.007232
405.237178	21631.451094	30.012250
405.972150	21657.587065	30.017268
406.272612	21698.554939	30.022285
406.949914	21726.764528	30.027303
407.181569	21751.367770	30.032320
407.298311	21797.030328	30.037338
407.942370	21825.128903	30.042356
408.259632	21866.211082	30.047373
408.951839	21900.925809	30.052391
409.304383	21926.737603	30.057408
409.588282	21965.971262	30.062426
409.916044	21991.788833	30.067444
410.324233	22029.631851	30.072461
411.092538	22055.464912	30.077479
411.486867	22085.872664	30.082496
411.551516	22134.261555	30.087514
412.149892	22160.826147	30.092532
412.796523	22200.713031	30.097549
413.039834	22218.055451	30.102567
413.415636	22262.164240	30.107584
413.668774	22279.956062	30.112602
414.383215	22319.202858	30.117620
414.365067	22346.535186	30.122637
414.911244	22381.426440	30.127655
415.489955	22416.714471	30.132672
415.550447	22455.428042	30.137690
416.458566	22476.363080	30.142708
416.734636	22527.001340	30.147725
416.947979	22551.413247	30.152743
417.405464	22589.845399	30.157760
417.761480	22622.248841	30.162778
418.257715	22657.413837	30.167796
418.308504	22697.250697	30.172813
418.924309	22732.914842	30.177831
419.213441	22764.568007	30.182848
419.340428	22818.849100	30.187866
420.136006	22860.305509	30.192884
420.501741	22894.928078	30.197901
421.106473	22930.607086	30.202919
421.671013	22961.995857	30.207936
421.949228	22995.497771	30.212954
422.312783	23026.719660	30.217972
422.806024	23059.733552	30.222989
422.953780	23084.789407	30.228007
423.696362	23112.938468	30.233024
423.765156	23154.578947	30.238042
424.563121	23192.131404	30.243060
424.670219	23221.912240	30.248077
424.917831	23257.690457	30.253095
425.181590	23287.379253	30.258112
425.521439	23333.280241	30.263130
426.135099	23367.924243	30.268148
426.086486	23424.319415	30.273165
426.638576	23467.728815	30.278183
427.540840	23500.346298	30.283200
427.464932	23552.400427	30.288218
428.307708	23596.864320	30.293236
429.125677	23646.965230	30.298253
429.004372	23683.754705	30.303271
429.720418	23713.486086	30.308288
430.201602	23761.607242	30.313306
430.542807	23795.723195	30.318324
431.047090	23837.132421	30.323341
431.461480	23882.442234	30.328359
431.719193	23916.994870	30.333376
431.766564	23974.482994	30.338394
432.760614	24016.518083	30.343412
433.375234	24057.099023	30.348429
433.702055	24098.800028	30.353447
434.080151	24137.433316	30.358464
434.336144	24183.066609	30.363482
435.203385	24223.915228	30.368500
435.675312	24262.599504	30.373517
435.989564	24298.424068	30.378535
436.619289	24329.560138	30.383552
436.949370	24377.837348	30.388570
437.654009	24407.488247	30.393588
438.192974	24448.634588	30.398605
438.327270	24496.026714	30.403623
438.962007	24518.144965	30.408640
439.303906	24563.544275	30.413658
439.336409	24597.384894	30.418676
439.873982	24642.089683	30.423693
440.122456	24685.549269	30.428711
441.175777	24715.518333	30.433728
441.225308	24768.463766	30.438746
441.806768	24801.491662	30.443764
442.414255	24842.867319	30.448781
442.585567	24882.917996	30.453799
443.265362	24916.850836	30.458816
443.167457	24964.516084	30.463834
444.062180	24994.158623	30.468852
444.356179	25041.200953	30.473869
444.720075	25084.450046	30.478887
445.330878	25127.689931	30.483904
445.628702	25170.218416	30.488922
446.011303	25217.571442	30.493940
446.563700	25259.824613	30.498957
447.139701	25292.684034	30.503975
447.769568	25335.498630	30.508992
448.036922	25372.585404	30.514010
448.735685	25410.894083	30.519028
448.956804	25453.795539	30.524045
449.564101	25488.470126	30.529063
450.041134	25519.163653	30.534080
450.538601	25560.928290	30.539098
451.044560	25585.832324	30.544116
451.459191	25623.828916	30.549133
451.858419	25654.321073	30.554151
452.281077	25685.112212	30.559168
452.415802	25719.568970	30.564186
452.900238	25749.927334	30.569204
453.652633	25785.313449	30.574221
453.631322	25824.309975	30.579239
454.376501	25849.540699	30.584256
454.540354	25903.631474	30.589274
455.162965	25935.430883	30.594292
455.721212	25972.224777	30.599309
455.633179	26017.229084	30.604327
456.208083	26051.162598	30.609344
456.595644	26097.911598	30.614362
457.221608	26138.706926	30.619380
457.846547	26185.533592	30.624397
457.958262	26222.900298	30.629415
458.750060	26259.511058	30.634432
458.950043	26318.158329	30.639450
459.464150	26354.250614	30.644468
459.945801	26404.842655	30.649485
460.195125	26452.180122	30.654503
461.077498	26492.369223	30.659520
461.291800	26536.678201	30.664538
461.852723	26588.948417	30.669556
462.759442	26630.619533	30.674573
463.235973	26671.563871	30.679591
463.263742	26705.557669	30.684608
463.787396	26747.503804	30.689626
464.249973	26801.286137	30.694644
464.398202	26842.629041	30.699661
464.987011	26897.255101	30.704679
465.716854	26938.290639	30.709696
466.067420	26990.148944	30.714714
466.340361	27037.357924	30.719732
467.172240	27083.465102	30.724749
467.152509	27130.136031	30.729767
467.882123	27179.045809	30.734784
468.348596	27227.582874	30.739802
468.579058	27275.711187	30.744820
469.445399	27316.608318	30.749837
469.818739	27371.851964	30.754855
470.461955	27414.237338	30.759872
470.702318	27459.197353	30.764890
471.204925	27505.899573	30.769908
471.967943	27541.785955	30.774925
472.381906	27600.058304	30.779943
472.703346	27640.450153	30.784960
473.155059	27689.315875	30.789978
473.998161	27737.012855	30.794996
474.521779	27780.027753	30.800013
474.731420	27823.596299	30.805031
475.686105	27861.110958	30.810048
475.443773	27907.978541	30.815066
476.040109	27946.789302	30.820084
476.810232	27986.009890	30.825101
476.936160	28040.703527	30.830119
477.648434	28085.107561	30.835136
478.215628	28125.090772	30.840154
478.296940	28178.820585	30.845172
479.104957	28221.698028	30.850189
479.348081	28268.890050	30.855207
480.026261	28317.656967	30.860224
480.401303	28355.656643	30.865242
480.855384	28405.445163	30.870260
481.535158	28442.536515	30.875277
481.856072	28498.779847	30.880295
482.327228	28537.088952	30.885312
482.907122	28574.477886	30.890330
482.854968	28626.322532	30.895348
483.584529	28657.361565	30.900365
484.133145	28707.624295	30.905383
484.205094	28743.898827	30.910400
484.785220	28797.570085	30.915418
485.431338	28852.754362	30.920436
485.962750	28889.773418	30.925453
486.064378	28934.627695	30.930471
487.038944	28982.082342	30.935488
487.767485	29032.278375	30.940506
487.735779	29079.354012	30.945524
488.422938	29112.814336	30.950541
488.748262	29166.074590	30.955559
489.291541	29213.582305	30.960576
490.226403	29264.000408	30.965594
490.357739	29311.961453	30.970612
490.875860	29348.841710	30.975629
491.267319	29405.965969	30.980647
492.024441	29450.290341	30.985664
492.803033	29495.819610	30.990682
493.090339	29545.635821	30.995700
493.654750	29586.244364	31.000717
494.056690	29636.928404	31.005735
494.901013	29679.907539	31.010752
495.204826	29716.388650	31.015770
495.663760	29758.251792	31.020788
496.517495	29801.049834	31.025805
496.575904	29843.783977	31.030823
497.155076	29894.814879	31.035840
498.034242	29932.182438	31.040858
498.431591	29982.647387	31.045876
498.775016	30025.300103	31.050893
499.255065	30077.707754	31.055911
499.843779	30113.817580	31.060928
500.335657	30158.856505	31.065946
500.823497	30205.221336	31.070964
501.441699	30250.851674	31.075981
501.596847	30301.275584	31.080999
502.007767	30348.297155	31.086016
502.776224	30387.356196	31.091034
502.906316	30439.936418	31.096052
503.580914	30483.097053	31.101069
504.256875	30542.260300	31.106087
504.532228	30583.045186	31.111104
505.195005	30629.738718	31.116122
505.534668	30687.386846	31.121140
506.111287	30732.425838	31.126157
506.292638	30791.592888	31.131175
506.926653	30832.959501	31.136192
507.870446	30888.867636	31.141210
508.027494	30950.172138	31.146228
508.569550	30982.369572	31.151245
508.843655	31038.486806	31.156263
509.676712	31084.907264	31.161280
510.130851	31137.458031	31.166298
510.598328	31193.780403	31.171316
511.109598	31241.623889	31.176333
511.568116	31289.624531	31.181351
512.042754	31347.094717	31.186368
512.338027	31398.804854	31.191386
512.772702	31451.284049	31.196404
513.679077	31504.310095	31.201421
514.150715	31569.852725	31.206439
514.446202	31619.326364	31.211456
515.022907	31667.642939	31.216474
515.466714	31726.441536	31.221492
515.947235	31772.776992	31.226509
516.464711	31825.792626	31.231527
517.041508	31874.620916	31.236544
517.488606	31918.529508	31.241562
517.738612	31974.735739	31.246580
518.384261	32024.764712	31.251597
518.944974	32069.036678	31.256615
519.465716	32130.707911	31.261632
520.219182	32182.218303	31.266650
520.531658	32239.863368	31.271668
521.234795	32272.831666	31.276685
521.919386	32334.864614	31.281703
522.428761	32379.720141	31.286720
523.035052	32428.819601	31.291738
522.894088	32477.724142	31.296756
523.812496	32531.792579	31.301773
524.100991	32588.852673	31.306791
524.492698	32642.055642	31.311808
525.214524	32695.336678	31.316826
525.653100	32762.425913	31.321844
526.419798	32817.915059	31.326861
526.832320	32864.848391	31.331879
527.344544	32915.485726	31.336896
527.810301	32974.496247	31.341914
527.807823	33042.517825	31.346932
528.798161	33098.762889	31.351949
529.287821	33164.731271	31.356967
529.981565	33224.462236	31.361984
530.877950	33287.179782	31.367002
531.147539	33342.049118	31.372020
531.856095	33393.418984	31.377037
532.255121	33452.830272	31.382055
532.712626	33506.940071	31.387072
533.358365	33561.085156	31.392090
533.865472	33630.059708	31.397108
534.574720	33675.125259	31.402125
534.940839	33744.593777	31.407143
535.552089	33792.809433	31.412160
536.191598	33856.410900	31.417178
536.580283	33917.438008	31.422196
537.204006	33965.951861	31.427213
537.740973	34026.639235	31.432231
538.574543	34081.310228	31.437248
539.117470	34132.495037	31.442266
539.648068	34193.089357	31.447284
540.109463	34239.898300	31.452301
540.786533	34295.545730	31.457319
541.568020	34342.491325	31.462336
541.978874	34386.579258	31.467354
542.372945	34454.818302	31.472372
543.073509	34501.427409	31.477389
543.481739	34554.453463	31.482407
543.784813	34610.271051	31.487424
544.455708	34669.543565	31.492442
544.806287	34721.342559	31.497460
545.439222	34771.299297	31.502477
545.937176	34832.617561	31.507495
546.517996	34886.231434	31.512512
546.986501	34945.964393	31.517530
547.440008	35007.158060	31.522548
547.975393	35066.299666	31.527565
548.910176	35124.883058	31.532583
549.419903	35188.368710	31.537600
550.048849	35239.921160	31.542618
550.270979	35304.231169	31.547636
550.922772	35360.028103	31.552653
551.771662	35417.017117	31.557671
552.007217	35464.986994	31.562688
552.664367	35519.233946	31.567706
552.915264	35573.384168	31.572724
553.706455	35628.745434	31.577741
554.203871	35670.294227	31.582759
554.623764	35730.640634	31.587776
554.966396	35779.007070	31.592794
555.457785	35846.323197	31.597812
556.048155	35893.036206	31.602829
556.176841	35953.586188	31.607847
556.800044	36025.394354	31.612864
557.609654	36078.623598	31.617882
558.085943	36143.405832	31.622900
558.368195	36208.750631	31.627917
558.837613	36264.918246	31.632935
559.542735	36329.360296	31.637952
560.319161	36397.388787	31.642970
561.040490	36471.505416	31.647988
561.825430	36524.086730	31.653005
562.151105	36593.052172	31.658023
562.087987	36655.258514	31.663040
562.926772	36714.377418	31.668058
563.807851	36791.139072	31.673076
564.429675	36856.448961	31.678093
565.103359	36915.630558	31.683111
565.842044	36980.915248	31.688128
566.402123	37041.441678	31.693146
567.082512	37113.983267	31.698164
567.461543	37164.654620	31.703181
568.333575	37228.775566	31.708199
568.787565	37294.932284	31.713216
569.329692	37351.810875	31.718234
570.108973	37421.345146	31.723252
570.182501	37474.813915	31.728269
570.606725	37533.944113	31.733287
571.380913	37605.768282	31.738304
572.086816	37657.598969	31.743322
572.763347	37732.987556	31.748340
573.022590	37794.377458	31.753357
574.298380	37856.110713	31.758375
574.526080	37922.275589	31.763392
575.156242	37964.464218	31.768410
576.097506	38035.063000	31.773428
576.418115	38083.287718	31.778445
577.181959	38141.082183	31.783463
577.379248	38203.433805	31.788480
578.012557	38262.781137	31.793498
578.637276	38317.556342	31.798516
579.094456	38385.484124	31.803533
580.085751	38445.568257	31.808551
580.509022	38517.381483	31.813568
581.321151	38574.976787	31.818586
582.114699	38627.783727	31.823604
582.402704	38682.565233	31.828621
583.066122	38745.425544	31.833639
583.573472	38808.690681	31.838656
584.236860	38859.606948	31.843674
584.752126	38917.441844	31.848692
584.925663	38975.175632	31.853709
586.119310	39030.363901	31.858727
586.215742	39100.165914	31.863744
587.139487	39155.506541	31.868762
587.609557	39215.300651	31.873780
588.167918	39271.993147	31.878797
588.645292	39326.802069	31.883815
588.813205	39395.943111	31.888832
589.864610	39455.411384	31.893850
590.068113	39519.572080	31.898868
590.867485	39583.296647	31.903885
591.153710	39643.040493	31.908903
591.776054	39709.651610	31.913920
592.455605	39763.803356	31.918938
593.199650	39826.123705	31.923956
593.746166	39879.682240	31.928973
594.644339	39936.727789	31.933991
595.301262	39997.352170	31.939008
595.636280	40043.000585	31.944026
596.224157	40099.002575	31.949044
596.567688	40157.027631	31.954061
597.476304	40209.472848	31.959079
597.655573	40283.176931	31.964096
598.526589	40337.898487	31.969114
599.001890	40413.972246	31.974132
599.383093	40469.791736	31.979149
599.896406	40541.541161	31.984167
600.404253	40601.260921	31.989184
600.985103	40665.536806	31.994202
601.372700	40742.548241	31.999220
601.788353	40812.720644	32.004237
602.557765	40887.860604	32.009255
603.050781	40956.947402	32.014272
604.068998	41047.651580	32.019290
604.468651	41118.563361	32.024308
605.105120	41193.287741	32.029325
605.828093	41262.195570	32.034343
606.198627	41339.325963	32.039360
607.304485	41411.962560	32.044378
608.007539	41484.833407	32.049396
608.229557	41561.452602	32.054413
609.230112	41635.139848	32.059431
609.384516	41711.032098	32.064448
610.160908	41783.813060	32.069466
610.526234	41864.053060	32.074484
611.206424	41933.197774	32.079501
612.287238	41996.644177	32.084519
612.812408	42079.608506	32.089536
613.952808	42149.729211	32.094554
614.632134	42217.485986	32.099572
615.213751	42285.963222	32.104589
615.985213	42348.821107	32.109607
616.532214	42419.524052	32.114624
617.148330	42484.210848	32.119642
617.716479	42544.634107	32.124660
618.190870	42607.144207	32.129677
618.927796	42668.442908	32.134695
619.566997	42748.717187	32.139712
620.052801	42806.101869	32.144730
620.653838	42876.860755	32.149748
621.343442	42955.485811	32.154765
621.917513	43007.119743	32.159783
622.385399	43078.706531	32.164800
622.834608	43153.318226	32.169818
623.742248	43226.670380	32.174836
624.349161	43292.867547	32.179853
625.148559	43349.302178	32.184871
625.657628	43424.577567	32.189888
626.287812	43492.640744	32.194906
626.718379	43553.601526	32.199924
627.301127	43633.074344	32.204941
628.204936	43701.231937	32.209959
628.992584	43775.979569	32.214976
629.181113	43843.400357	32.219994
630.381657	43901.765783	32.225012
630.772394	43972.538351	32.230029
631.155490	44031.531982	32.235047
632.298249	44106.919983	32.240064
632.763394	44171.511301	32.245082
633.186580	44238.724185	32.250100
633.782516	44295.852091	32.255117
634.227584	44361.432524	32.260135
634.827140	44420.442087	32.265152
635.643479	44487.126661	32.270170
636.307346	44551.414862	32.275188
636.319310	44611.036914	32.280205
637.127378	44678.266634	32.285223
637.591123	44756.519819	32.290240
638.187446	44827.807857	32.295258
639.175857	44902.267840	32.300276
639.578998	44982.281300	32.305293
640.036230	45057.136061	32.310311
640.829202	45138.468732	32.315328
641.179501	45208.797942	32.320346
642.179335	45281.978688	32.325364
642.845217	45367.097307	32.330381
643.792756	45446.252198	32.335399
643.924146	45522.681563	32.340416
644.551295	45594.340009	32.345434
645.354430	45662.710837	32.350452
646.021416	45750.657169	32.355469
646.880675	45825.521095	32.360487
647.585458	45910.288372	32.365504
648.228840	45985.693889	32.370522
649.048488	46044.113198	32.375540
649.239016	46125.669783	32.380557
650.218662	46205.517260	32.385575
650.634716	46284.413071	32.390592
651.128611	46356.570124	32.395610
652.275163	46443.234039	32.400628
652.270454	46531.165646	32.405645
653.241733	46600.999405	32.410663
654.035144	46686.892333	32.415680
654.387970	46765.601655	32.420698
655.449034	46847.743644	32.425716
655.786538	46937.512111	32.430733
656.763509	47008.836978	32.435751
657.597862	47091.447007	32.440768
657.933382	47173.028311	32.445786
659.008429	47245.702088	32.450804
659.421972	47338.201002	32.455821
660.093983	47402.308065	32.460839
660.391438	47474.050261	32.465856
661.599183	47562.828198	32.470874
662.134169	47639.827761	32.475892
662.866792	47711.644129	32.480909
663.581381	47793.989634	32.485927
664.387962	47877.450874	32.490944
665.037967	47942.450819	32.495962
665.760927	48024.129571	32.500980
666.039710	48110.098262	32.505997
666.824593	48181.490878	32.511015
667.729470	48264.861753	32.516032
668.133422	48335.127334	32.521050
669.081151	48421.912105	32.526068
669.388596	48498.867498	32.531085
670.181717	48577.167207	32.536103
670.927529	48642.981134	32.541120
671.316261	48733.599127	32.546138
672.537286	48812.466973	32.551156
672.718992	48890.480644	32.556173
673.773044	48960.555698	32.561191
674.602759	49037.051015	32.566208
674.944157	49118.911255	32.571226
675.622136	49194.721685	32.576244
675.970845	49274.310550	32.581261
676.973288	49347.879188	32.586279
677.362379	49423.097166	32.591296
677.962415	49503.400247	32.596314
678.842848	49574.299011	32.601332
679.391312	49649.854723	32.606349
680.267897	49727.396776	32.611367
681.032495	49805.949409	32.616384
681.085778	49876.761874	32.621402
682.121877	49952.039120	32.626420
682.455232	50036.030213	32.631437
683.038290	50108.802564	32.636455
683.962494	50189.121202	32.641472
684.379484	50276.188492	32.646490
685.362017	50356.321300	32.651508
686.031505	50450.511089	32.656525
686.766825	50535.379094	32.661543
687.255170	50618.210004	32.666560
687.941710	50702.259271	32.671578
688.909997	50772.004504	32.676596
689.827920	50860.772989	32.681613
690.285926	50941.734102	32.686631
690.894424	51022.898077	32.691648
691.879055	51116.881043	32.696666
692.599220	51184.104002	32.701684
693.243474	51283.286342	32.706701
694.131979	51359.212579	32.711719
694.632209	51429.833591	32.716736
695.225112	51517.047920	32.721754
695.848491	51607.384717	32.726772
696.625802	51688.561452	32.731789
697.249066	51776.359442	32.736807
697.936337	51867.533417	32.741824
698.664501	51955.649690	32.746842
699.267877	52036.945095	32.751860
699.763707	52117.620555	32.756877
700.582715	52222.717295	32.761895
701.407864	52311.153963	32.766912
701.861870	52403.992666	32.771930
702.578208	52496.933721	32.776948
703.325622	52590.969362	32.781965
704.190865	52679.982299	32.786983
704.880510	52776.410183	32.792000
705.877319	52865.522239	32.797018
706.602821	52949.088287	32.802036
707.058967	53040.470233	32.807053
707.656618	53142.335873	32.812071
708.564473	53227.003847	32.817088
709.320008	53320.144499	32.822106
709.951538	53415.669037	32.827124
710.870025	53505.536165	32.832141
711.635970	53592.686904	32.837159
712.128656	53682.991727	32.842176
712.595039	53775.215702	32.847194
713.732794	53863.576077	32.852212
714.239936	53955.358203	32.857229
714.690187	54049.146718	32.862247
715.555735	54139.556230	32.867264
716.170028	54235.946880	32.872282
716.898081	54329.008401	32.877300
717.762289	54423.867513	32.882317
718.283308	54523.617389	32.887335
719.393205	54613.432639	32.892352
719.667623	54717.388097	32.897370
720.476932	54801.011333	32.902388
721.194445	54905.911754	32.907405
721.781190	55004.541133	32.912423
722.563323	55093.660882	32.917440
723.255825	55201.896875	32.922458
724.191248	55292.319060	32.927476
724.784935	55389.091537	32.932493
725.624590	55474.159563	32.937511
726.780675	55556.502810	32.942528
727.115907	55650.298986	32.947546
727.750613	55731.042107	32.952564
728.397353	55815.966585	32.957581
729.093100	55913.565131	32.962599
729.995013	55993.822804	32.967616
730.784371	56086.787661	32.972634
731.019331	56178.208069	32.977652
731.560392	56265.433061	32.982669
732.237197	56365.021091	32.987687
733.296269	56457.557608	32.992704
733.901448	56565.790196	32.997722
734.670521	56667.588762	33.002740
735.376395	56760.614805	33.007757
735.956243	56863.696845	33.012775
737.112285	56963.992158	33.017792
737.295365	57066.799644	33.022810
738.234032	57158.841159	33.027828
738.859876	57263.168848	33.032845
739.588742	57384.143914	33.037863
740.721707	57471.099321	33.042880
741.379621	57578.241747	33.047898
742.133502	57674.461672	33.052916
742.883104	57783.574304	33.057933
743.469034	57890.774541	33.062951
744.378605	57990.616532	33.067968
745.503342	58105.621782	33.072986
746.041476	58203.927444	33.078004
747.174778	58305.174840	33.083021
748.025315	58396.516185	33.088039
748.931649	58492.499944	33.093056
749.652041	58593.248325	33.098074
750.217544	58681.168629	33.103092
751.409219	58781.593529	33.108109
751.689877	58875.717182	33.113127
752.621013	58977.702889	33.118144
753.203806	59064.098939	33.123162
754.129597	59157.706408	33.128180
754.894479	59263.772060	33.133197
755.559357	59364.141640	33.138215
756.563365	59457.099249	33.143232
756.998642	59566.734877	33.148250
758.108586	59657.223746	33.153268
758.955647	59754.885461	33.158285
759.300015	59851.290950	33.163303
760.245985	59939.678353	33.168320
760.799735	60041.144077	33.173338
761.565528	60143.801336	33.178356
762.363504	60241.732638	33.183373
762.810050	60351.933135	33.188391
763.974926	60443.155885	33.193408
764.232452	60545.469469	33.198426
765.212233	60656.006867	33.203444
765.930464	60745.579415	33.208461
766.675130	60873.082670	33.213479
767.619002	60970.961745	33.218496
768.220907	61074.605182	33.223514
769.097925	61177.723286	33.228532
770.128222	61279.659911	33.233549
770.458873	61389.524915	33.238567
771.634584	61489.397011	33.243584
772.058737	61593.382185	33.248602
772.694268	61701.826872	33.253620
773.640226	61795.803421	33.258637
774.320319	61899.829985	33.263655
775.416078	62005.596042	33.268672
776.349848	62114.221125	33.273690
776.527695	62210.798031	33.278708
777.767277	62297.554253	33.283725
778.186739	62397.145010	33.288743
779.024037	62485.112633	33.293760
779.602949	62593.400731	33.298778
779.921659	62696.094187	33.303796
780.925790	62787.828054	33.308813
781.599095	62895.944106	33.313831
782.143349	63008.241291	33.318848
783.000029	63120.038617	33.323866
783.882659	63229.196369	33.328884
784.500552	63344.428822	33.333901
785.196847	63460.654010	33.338919
786.219797	63567.963533	33.343936
786.977575	63679.761283	33.348954
787.682891	63798.351008	33.353972
788.752686	63910.294353	33.358989
789.521419	64028.413453	33.364007
790.267319	64132.130648	33.369024
791.073363	64250.099448	33.374042
792.001782	64362.176080	33.379060
792.963406	64471.833031	33.384077
793.564501	64595.280458	33.389095
794.561200	64700.172733	33.394112
795.169114	64816.179916	33.399130
795.931820	64939.798624	33.404148
796.870461	65035.953113	33.409165
797.494788	65158.976490	33.414183
798.391124	65278.567173	33.419200
799.594978	65394.580153	33.424218
800.192953	65512.546267	33.429236
800.916213	65621.660770	33.434253
801.843793	65735.262159	33.439271
802.552569	65847.117588	33.444288
803.581095	65966.816782	33.449306
804.299974	66088.040887	33.454324
805.317573	66190.041744	33.459341
805.954993	66315.225545	33.464359
806.419993	66433.073429	33.469376
807.491709	66543.589168	33.474394
807.947070	66661.155432	33.479412
809.234543	66778.395059	33.484429
809.792547	66904.132884	33.489447
810.937564	67024.703947	33.494464
811.672510	67134.292226	33.499482
812.447686	67254.843588	33.504500
813.492549	67364.147877	33.509517
813.889408	67482.133024	33.514535
815.018281	67595.180095	33.519552
815.958761	67710.832158	33.524570
816.720530	67839.077142	33.529588
817.730575	67945.924440	33.534605
818.291248	68065.105985	33.539623
819.103281	68181.281344	33.544640
819.947882	68291.363289	33.549658
820.571895	68421.581943	33.554676
821.712893	68527.386247	33.559693
822.330417	68645.025238	33.564711
823.496666	68755.676017	33.569728
824.478726	68869.272634	33.574746
825.054548	68986.686469	33.579764
825.979543	69094.660109	33.584781
826.705739	69212.334845	33.589799
827.465959	69319.786788	33.594816
828.386224	69424.860671	33.599834
828.958800	69548.816053	33.604852
829.780980	69659.958400	33.609869
830.687174	69786.212139	33.614887
831.915670	69880.974994	33.619904
832.372041	69994.569703	33.624922
833.069244	70097.913319	33.629940
834.091120	70198.693440	33.634957
834.609224	70312.791801	33.639975
835.482508	70421.836674	33.644992
836.346965	70532.249386	33.650010
836.854557	70637.941278	33.655028
838.016910	70751.619254	33.660045
838.679314	70864.318195	33.665063
839.447916	70980.149211	33.670080
840.402560	71099.402672	33.675098
840.865634	71225.630669	33.680116
842.167353	71333.882112	33.685133
843.085069	71462.496144	33.690151
843.700823	71579.272571	33.695168
844.703594	71692.128225	33.700186
845.260488	71818.318877	33.705204
846.111987	71934.995000	33.710221
846.732463	72056.971286	33.715239
847.659617	72186.068664	33.720256
848.686045	72311.179057	33.725274
849.079645	72437.944170	33.730292
850.132941	72561.129121	33.735309
851.353246	72694.652009	33.740327
851.742469	72827.579592	33.745344
853.133347	72959.482266	33.750362
853.973075	73087.012144	33.755380
854.747263	73201.070750	33.760397
855.021282	73337.947730	33.765415
856.542978	73475.789182	33.770432
857.276424	73606.900159	33.775450
857.833450	73736.491672	33.780468
859.172022	73867.946830	33.785485
860.056137	73999.250266	33.790503
860.583076	74135.514902	33.795520
861.747133	74256.661014	33.800538
862.107761	74395.952513	33.805556
863.495880	74518.561896	33.810573
864.271781	74659.259977	33.815591
865.227478	74785.009728	33.820608
866.092945	74916.745483	33.825626
866.796826	75054.194542	33.830644
867.880137	75180.317573	33.835661
868.634024	75308.582941	33.840679
869.484420	75439.793046	33.845696
870.423237	75579.312646	33.850714
871.408409	75709.331991	33.855732
872.360991	75845.479898	33.860749
873.253451	75967.464623	33.865767
873.926460	76099.429014	33.870784
874.927485	76229.176824	33.875802
875.562788	76368.454327	33.880820
876.615183	76501.939609	33.885837
877.438255	76642.414826	33.890855
878.638027	76767.167767	33.895872
879.136603	76893.156917	33.900890
880.229080	77031.325651	33.905908
880.784273	77157.104527	33.910925
881.797655	77298.962930	33.915943
882.950245	77441.899809	33.920960
883.808781	77563.146202	33.925978
884.663645	77693.647813	33.930996
885.779672	77831.286284	33.936013
886.259307	77960.858427	33.941031
887.213504	78088.935939	33.946048
888.134654	78224.471060	33.951066
888.963019	78360.231087	33.956084
889.838910	78479.430109	33.961101
890.667033	78597.783712	33.966119
891.525777	78721.667788	33.971136
892.850221	78847.259364	33.976154
893.429344	78974.834655	33.981172
894.258463	79092.830135	33.986189
895.132506	79210.711266	33.991207
895.666249	79342.319322	33.996224
897.044929	79463.989708	34.001242
897.521883	79602.971937	34.006260
898.339808	79729.790857	34.011277
899.213058	79858.524424	34.016295
899.830292	80005.475584	34.021312
901.066721	80143.544789	34.026330
901.682274	80276.068348	34.031348
903.190267	80418.073403	34.036365
903.899354	80552.639089	34.041383
904.690667	80686.983211	34.046400
905.795975	80823.142431	34.051418
906.606658	80964.209744	34.056436
907.548465	81106.451913	34.061453
908.272538	81240.139835	34.066471
909.135901	81385.705385	34.071488
910.404565	81528.737543	34.076506
911.190579	81663.632371	34.081524
912.052359	81809.219862	34.086541
913.090392	81954.601991	34.091559
914.087319	82091.760991	34.096576
915.113534	82230.870886	34.101594
915.913668	82376.301359	34.106612
916.872085	82513.020057	34.111629
917.638564	82660.096501	34.116647
918.468277	82814.262045	34.121664
919.435575	82949.571005	34.126682
920.262121	83099.095116	34.131700
921.478875	83247.037220	34.136717
922.365543	83379.850272	34.141735
923.551345	83536.891124	34.146752
924.792198	83667.432827	34.151770
925.421078	83809.249995	34.156788
926.465659	83939.243604	34.161805
927.584038	84082.930236	34.166823
928.649030	84221.609167	34.171840
929.934552	84353.292565	34.176858
930.446916	84495.057271	34.181876
931.489155	84623.043048	34.186893
932.844126	84759.329829	34.191911
933.441536	84901.519532	34.196928
934.411918	85024.849838	34.201946
935.539517	85162.992536	34.206964
936.037008	85289.895167	34.211981
936.911980	85420.608473	34.216999
938.182273	85567.056911	34.222016
939.082436	85704.500105	34.227034
939.723790	85841.619905	34.232052
940.629907	85982.961539	34.237069
941.695918	86119.196478	34.242087
942.747431	86257.934043	34.247104
943.452303	86396.217205	34.252122
944.717877	86535.313331	34.257140
945.398133	86666.426469	34.262157
946.271352	86805.329635	34.267175
947.276656	86942.718399	34.272192
948.539065	87080.888077	34.277210
949.273413	87224.486676	34.282228
949.882427	87368.758656	34.287245
950.911218	87501.375487	34.292263
951.605208	87645.388310	34.297280
952.664458	87773.951672	34.302298
953.993908	87911.203875	34.307316
954.898876	88048.166361	34.312333
955.644950	88182.384158	34.317351
956.031898	88312.333582	34.322368
956.800729	88447.188264	34.327386
958.108714	88580.948354	34.332404
958.899418	88723.394960	34.337421
959.927384	88873.308652	34.342439
960.862988	89019.536430	34.347456
961.913295	89159.506269	34.352474
962.898660	89306.986943	34.357492
963.567621	89449.413715	34.362509
964.578073	89596.575600	34.367527
965.556269	89745.806853	34.372544
966.624459	89896.486075	34.377562
967.731600	90039.141342	34.382580
968.489967	90191.626698	34.387597
969.658838	90346.342487	34.392615
970.435099	90502.111489	34.397632
971.681839	90655.019003	34.402650
972.806202	90803.941530	34.407668
973.468333	90965.124618	34.412685
974.317205	91102.132846	34.417703
975.088188	91269.223885	34.422720
976.256761	91428.237740	34.427738
977.306902	91576.481106	34.432756
978.170277	91747.503197	34.437773
979.308638	91901.025124	34.442791
979.893452	92071.019594	34.447808
981.052957	92238.780929	34.452826
982.184786	92396.300836	34.457844
982.803191	92565.122278	34.462861
984.238053	92725.442417	34.467879
984.847019	92902.084559	34.472896
985.872823	93057.474257	34.477914
986.984493	93231.003828	34.482932
987.719304	93404.426046	34.487949
988.774979	93568.700773	34.492967
989.461889	93742.481429	34.497984
990.842228	93913.116725	34.503002
991.676351	94081.204019	34.508020
992.458014	94271.544032	34.513037
993.880956	94428.098390	34.518055
994.701356	94613.959446	34.523072
995.877799	94777.000602	34.528090
996.856415	94954.457236	34.533108
997.892810	95130.006584	34.538125
999.016209	95290.394957	34.543143
1000.110286	95470.450510	34.548160
1001.127039	95642.683431	34.553178
1002.285799	95810.545224	34.558196
1003.313155	95985.095613	34.563213
1004.439584	96152.021850	34.568231
1005.455267	96314.536294	34.573248
1006.653368	96475.439044	34.578266
1007.572889	96641.199998	34.583284
1008.394741	96815.442003	34.588301
1009.767492	96973.786904	34.593319
1010.698277	97142.556295	34.598336
1011.649249	97301.916259	34.603354
1012.661554	97469.224668	34.608372
1013.416670	97635.500505	34.613389
1014.461149	97799.621474	34.618407
1015.847943	97979.672020	34.623424
1016.352968	98134.489553	34.628442
1017.287374	98298.720602	34.633460
1018.606897	98477.298078	34.638477
1019.720446	98634.088246	34.643495
1020.737055	98785.900302	34.648512
1021.634785	98938.226740	34.653530
1022.758878	99088.459084	34.658548
1023.476884	99247.135446	34.663565
1024.669973	99403.265118	34.668583
1025.574427	99567.091482	34.673600
1026.588936	99723.911087	34.678618
1027.455795	99880.407852	34.683636
1027.838295	100057.030409	34.688653
1029.208712	100226.159196	34.693671
1029.931828	100396.630740	34.698688
1031.096744	100578.927038	34.703706
1032.351610	100751.009829	34.708724
1032.831934	100934.447536	34.713741
1034.171497	101106.050174	34.718759
1034.936492	101292.336866	34.723776
1035.889238	101466.975369	34.728794
1037.278364	101658.150813	34.733812
1037.931629	101840.293710	34.738829
1038.924395	102029.948186	34.743847
1040.188093	102215.937472	34.748864
1041.104787	102406.519060	34.753882
1042.277466	102606.462563	34.758900
1043.305433	102794.875764	34.763917
1044.120279	102978.525931	34.768935
1045.259322	103182.234281	34.773952
1046.553902	103377.414536	34.778970
1047.639722	103554.647566	34.783988
1048.846373	103755.088170	34.789005
1049.672875	103946.791395	34.794023
1050.560973	104146.629115	34.799040
1051.788372	104342.536887	34.804058
1052.700118	104527.657332	34.809076
1053.894594	104732.654040	34.814093
1055.359013	104916.039416	34.819111
1056.315208	105118.862171	34.824128
1057.637414	105311.633228	34.829146
1058.833439	105486.834652	34.834164
1059.552088	105685.483533	34.839181
1060.808988	105887.819180	34.844199
1061.975985	106078.810338	34.849216
1063.027171	106263.299271	34.854234
1064.532376	106449.107635	34.859252
1065.097763	106641.000228	34.864269
1066.361312	106825.875914	34.869287
1067.445500	107027.463498	34.874304
1068.235677	107212.534116	34.879322
1069.569367	107404.431819	34.884340
1070.416752	107594.600040	34.889357
1071.806931	107784.679865	34.894375
1072.678248	107973.098865	34.899392
1073.942851	108160.326850	34.904410
1075.081322	108360.610827	34.909428
1075.964575	108552.312529	34.914445
1077.235778	108740.974778	34.919463
1078.155668	108933.496459	34.924480
1078.958531	109131.764282	34.929498
1080.251672	109318.349557	34.934516
1081.161168	109520.314006	34.939533
1082.105886	109712.799106	34.944551
1083.289030	109911.111076	34.949568
1084.212225	110122.590819	34.954586
1085.376648	110305.657287	34.959604
1086.221412	110510.692616	34.964621
1087.239693	110708.809615	34.969639
1088.379177	110912.291778	34.974656
1089.099015	111120.367229	34.979674
1090.784990	111306.559103	34.984692
1091.651907	111499.741020	34.989709
1092.604827	111686.563377	34.994727
1094.002571	111862.292177	34.999744
1095.420740	112062.848429	35.004762
1096.629861	112251.570486	35.009780
1097.265888	112443.099613	35.014797
1098.315928	112635.334391	35.019815
1099.462883	112828.834002	35.024832
1100.452683	113022.272260	35.029850
1101.513841	113217.752401	35.034868
1102.505078	113412.726048	35.039885
1103.769058	113605.945660	35.044903
1104.681612	113804.634375	35.049920
1105.515052	114021.150347	35.054938
1106.734726	114214.710878	35.059956
1107.944232	114424.415103	35.064973
1109.040039	114633.189483	35.069991
1110.580204	114842.880167	35.075008
1111.521228	115050.086868	35.080026
1112.503566	115249.825822	35.085044
1113.595269	115454.603339	35.090061
1114.518133	115671.623984	35.095079
1115.963942	115880.108977	35.100096
1116.797302	116094.524970	35.105114
1118.355403	116304.122140	35.110132
1119.184191	116509.039407	35.115149
1120.252062	116726.576268	35.120167
1121.571798	116943.148203	35.125184
1122.570620	117158.457097	35.130202
1123.950376	117371.259202	35.135220
1124.885084	117583.680314	35.140237
1126.194427	117801.540183	35.145255
1127.555769	118022.396106	35.150272
1128.600160	118233.397403	35.155290
1129.842268	118444.937751	35.160308
1131.194598	118660.642911	35.165325
1131.847613	118863.996761	35.170343
1133.250912	119083.548701	35.175360
1134.290511	119316.961640	35.180378
1135.489806	119517.454696	35.185396
1136.905027	119731.915590	35.190413
1137.919264	119938.879326	35.195431
1138.892800	120153.517704	35.200448
1140.365479	120375.500878	35.205466
1141.569611	120585.111557	35.210484
1142.624538	120798.283911	35.215501
1143.776013	121014.039645	35.220519
1144.887743	121219.653030	35.225536
1146.186960	121440.773178	35.230554
1147.615715	121652.141109	35.235572
1148.613147	121866.065673	35.240589
1149.872599	122068.923262	35.245607
1151.145394	122279.345648	35.250624
1152.300297	122489.852375	35.255642
1153.491734	122694.854506	35.260660
1154.650808	122905.008630	35.265677
1155.744214	123119.813435	35.270695
1156.799966	123318.011473	35.275712
1157.462387	123523.436231	35.280730
1158.769968	123743.051275	35.285748
1160.017664	123961.207702	35.290765
1161.546697	124179.268505	35.295783
1162.701681	124386.569443	35.300800
1163.681761	124611.618563	35.305818
1164.782581	124814.254783	35.310836
1165.842250	125026.683398	35.315853
1166.960491	125238.102571	35.320871
1168.543646	125431.094318	35.325888
1169.146304	125641.359462	35.330906
1170.510982	125832.653508	35.335924
1171.362646	126042.715484	35.340941
1172.658344	126253.237821	35.345959
1174.031551	126451.885476	35.350976
1174.632437	126662.386057	35.355994
1175.807462	126863.882887	35.361012
1176.792707	127080.203821	35.366029
1177.802677	127299.526115	35.371047
1179.241857	127514.672340	35.376064
1180.210302	127741.153279	35.381082
1181.272802	127958.380177	35.386100
1182.669465	128185.744202	35.391117
1183.933984	128406.578612	35.396135
1184.919458	128629.945085	35.401152
1185.977136	128858.143244	35.406170
1187.366406	129083.132039	35.411188
1188.455006	129314.433918	35.416205
1189.229020	129550.809095	35.421223
1190.772515	129772.709805	35.426240
1191.668964	130024.114504	35.431258
1192.835393	130250.327339	35.436276
1194.061421	130491.730599	35.441293
1195.047848	130742.821903	35.446311
1196.943085	130982.952065	35.451328
1198.191432	131227.678421	35.456346
1199.351807	131461.861668	35.461364
1200.672014	131701.699326	35.466381
1201.677684	131941.286533	35.471399
1202.920380	132176.095230	35.476416
1203.927484	132418.994404	35.481434
1205.190352	132663.970186	35.486452
1206.531388	132903.318965	35.491469
1207.829622	133151.664702	35.496487
1209.097173	133404.530521	35.501504
1210.368255	133644.276656	35.506522
1211.749929	133884.906377	35.511540
1213.195597	134117.870061	35.516557
1214.659952	134360.112347	35.521575
1215.673629	134605.143959	35.526592
1216.878980	134844.618187	35.531610
1218.214931	135079.394422	35.536628
1219.729147	135321.635568	35.541645
1220.702464	135560.595529	35.546663
1221.825643	135792.407304	35.551680
1223.227307	136036.155643	35.556698
1224.559071	136272.145486	35.561716
1225.995902	136507.371609	35.566733
1226.962808	136756.674193	35.571751
1228.302148	136977.707093	35.576768
1229.597257	137231.409174	35.581786
1230.710285	137455.183208	35.586804
1232.042858	137685.959237	35.591821
1232.853396	137926.877584	35.596839
1234.107864	138160.484516	35.601856
1235.560167	138412.559283	35.606874
1236.366003	138653.648421	35.611892
1237.797488	138888.321537	35.616909
1239.042947	139139.015809	35.621927
1240.486429	139372.815406	35.626944
1241.480076	139626.965687	35.631962
1242.937452	139863.999658	35.636980
1244.250015	140108.083822	35.641997
1245.154454	140361.975346	35.647015
1246.620680	140602.119531	35.652032
1247.938188	140849.682460	35.657050
1249.075035	141082.796269	35.662068
1250.455665	141318.026997	35.667085
1251.361925	141544.651697	35.672103
1252.618563	141772.969860	35.677120
1253.661022	142005.813820	35.682138
1254.775146	142237.290667	35.687156
1256.234342	142473.860364	35.692173
1257.075484	142716.011905	35.697191
1258.209015	142963.417385	35.702208
1259.511514	143201.602995	35.707226
1260.558217	143446.325179	35.712244
1261.981758	143690.669745	35.717261
1263.128750	143950.025528	35.722279
1264.602198	144201.910690	35.727296
1265.923174	144457.081954	35.732314
1266.780876	144706.117695	35.737332
1268.223428	144959.978951	35.742349
1269.352754	145219.676615	35.747367
1271.040472	145476.684107	35.752384
1271.810780	145746.793229	35.757402
1273.023667	146016.057625	35.762420
1274.656052	146265.331225	35.767437
1275.441743	146540.516546	35.772455
1277.001260	146799.926200	35.777472
1278.470119	147077.856171	35.782490
1279.628487	147340.341683	35.787508
1280.739362	147611.752721	35.792525
1282.199731	147895.055001	35.797543
1283.413313	148152.882695	35.802560
1284.568511	148433.969364	35.807578
1285.988541	148707.772482	35.812596
1287.541856	148982.215109	35.817613
1288.583588	149273.828402	35.822631
1290.055972	149549.975446	35.827648
1291.409815	149827.919781	35.832666
1292.605336	150101.427812	35.837684
1294.342843	150370.802243	35.842701
1295.448647	150653.372412	35.847719
1296.638447	150929.817310	35.852736
1298.320370	151206.614138	35.857754
1299.428738	151491.612739	35.862772
1301.029738	151764.875550	35.867789
1302.135542	152043.511391	35.872807
1303.701325	152316.441508	35.877824
1305.104115	152595.932859	35.882842
1306.190489	152865.901920	35.887860
1307.912207	153127.878199	35.892877
1309.261280	153413.954865	35.897895
1310.468352	153682.324133	35.902912
1311.983039	153954.969873	35.907930
1313.026957	154223.154204	35.912948
1314.402593	154489.382835	35.917965
1315.546836	154776.860652	35.922983
1317.107308	155054.846844	35.928000
1318.233841	155326.373911	35.933018
1319.635668	155605.937794	35.938036
1320.810220	155877.042103	35.943053
1322.016450	156156.883224	35.948071
1323.797495	156421.966971	35.953088
1325.276379	156696.692661	35.958106
1326.235623	156987.439228	35.963124
1327.777333	157255.790207	35.968141
1329.177910	157537.473675	35.973159
1330.425957	157801.145034	35.978176
1331.968078	158073.560868	35.983194
1333.478600	158353.024501	35.988212
1334.727294	158622.079974	35.993229
1335.829641	158896.806768	35.998247
1337.284665	159157.940865	36.003264
1338.320800	159417.724986	36.008282
1339.262874	159668.265198	36.013300
1341.212729	159920.302315	36.018317
1342.340921	160195.198452	36.023335
1343.083685	160450.559199	36.028352
1344.635284	160720.111188	36.033370
1345.967092	160991.426658	36.038388
1347.648693	161250.303652	36.043405
1348.702165	161532.148028	36.048423
1349.890188	161780.363982	36.053440
1351.434966	162065.264447	36.058458
1352.540689	162338.897000	36.063476
1354.117135	162602.455916	36.068493
1355.038461	162891.829423	36.073511
1356.279345	163166.624905	36.078528
1357.890104	163443.264166	36.083546
1358.936800	163736.543141	36.088564
1360.612863	164012.959597	36.093581
1361.496947	164310.697383	36.098599
1362.741332	164598.075089	36.103616
1364.404393	164894.140228	36.108634
1365.643728	165199.133696	36.113652
1367.390270	165482.513644	36.118669
1368.583888	165779.106461	36.123687
1369.923611	166086.589113	36.128704
1371.212055	166378.006144	36.133722
1372.831587	166689.062958	36.138740
1374.144524	166981.139717	36.143757
1375.495479	167274.620556	36.148775
1376.478848	167584.938628	36.153792
1378.370838	167880.237351	36.158810
1379.636154	168201.793493	36.163828
1381.199739	168506.388154	36.168845
1382.839051	168808.827892	36.173863
1384.070829	169109.129074	36.178880
1385.402154	169412.968786	36.183898
1386.927869	169708.695266	36.188916
1388.387668	170019.408102	36.193933
1390.131249	170330.558342	36.198951
1391.422560	170633.587924	36.203968
1392.837894	170924.137705	36.208986
1393.932530	171231.835438	36.214004
1395.528912	171525.036595	36.219021
1397.289741	171839.442697	36.224039
1398.072489	172142.121975	36.229056
1399.878772	172448.352256	36.234074
1401.225894	172763.975003	36.239092
1403.029602	173060.742783	36.244109
1404.348039	173363.366718	36.249127
1405.470398	173665.453900	36.254144
1407.004538	173961.726133	36.259162
1408.469060	174273.075432	36.264180
1409.859998	174578.664637	36.269197
1411.222796	174883.422829	36.274215
1412.256226	175194.861974	36.279232
1413.799579	175501.523199	36.284250
1415.039913	175815.368756	36.289268
1416.637697	176128.713058	36.294285
1417.968046	176442.344672	36.299303
1419.513589	176753.137946	36.304320
1420.992890	177064.604054	36.309338
1422.079479	177378.814883	36.314356
1423.531089	177691.964734	36.319373
1425.243418	178012.053805	36.324391
1426.836249	178319.371480	36.329408
1428.061536	178624.200718	36.334426
1429.541346	178948.941211	36.339444
1430.917739	179241.476204	36.344461
1432.340207	179539.348554	36.349479
1433.744569	179844.777364	36.354496
1435.160638	180126.662228	36.359514
1436.232009	180433.114127	36.364532
1437.658924	180730.802207	36.369549
1439.038513	181023.562496	36.374567
1440.633305	181333.652018	36.379584
1442.336448	181645.781635	36.384602
1443.530331	181953.783327	36.389620
1444.671728	182256.223427	36.394637
1446.454040	182557.175833	36.399655
1447.505744	182874.789293	36.404672
1449.139919	183190.518691	36.409690
1450.595478	183512.625893	36.414708
1451.711316	183829.117387	36.419725
1453.093395	184154.858027	36.424743
1454.376162	184483.752213	36.429760
1455.929182	184803.324989	36.434778
1457.289483	185141.704794	36.439796
1458.934774	185477.792849	36.444813
1460.526464	185815.097663	36.449831
1461.684172	186155.357641	36.454848
1463.284884	186486.419798	36.459866
1464.383128	186822.453973	36.464884
1465.769311	187172.164469	36.469901
1467.505286	187501.712333	36.474919
1469.140045	187860.855537	36.479936
1470.631526	188198.533795	36.484954
1471.405821	188544.583641	36.489972
1473.442632	188890.414236	36.494989
1475.347059	189234.466180	36.500007
1476.197338	189592.289861	36.505024
1478.461820	189937.568535	36.510042
1479.397375	190280.250647	36.515060
1481.059118	190641.183636	36.520077
1482.767535	190990.013178	36.525095
1483.968980	191343.435098	36.530112
1485.557663	191695.563707	36.535130
1487.264816	192049.007726	36.540148
1488.868246	192398.230846	36.545165
1490.823811	192740.834492	36.550183
1492.240233	193095.843252	36.555200
1494.087353	193436.348594	36.560218
1495.681599	193788.145451	36.565236
1496.618626	194124.805939	36.570253
1497.980977	194467.212371	36.575271
1499.455801	194831.768111	36.580288
1501.152919	195168.181578	36.585306
1502.912167	195522.766449	36.590324
1504.375700	195872.539735	36.595341
1506.190295	196213.865103	36.600359
1507.584616	196571.918415	36.605376
1509.430696	196903.606158	36.610394
1510.588720	197257.347597	36.615412
1511.807849	197598.270687	36.620429
1513.616308	197943.770247	36.625447
1514.997220	198290.243640	36.630464
1517.077502	198638.075999	36.635482
1518.209325	198983.273696	36.640500
1519.663190	199336.482010	36.645517
1521.211447	199677.526220	36.650535
1522.645907	200025.916689	36.655552
1524.083540	200372.619758	36.660570
1525.978069	200711.262988	36.665588
1527.396422	201062.695726	36.670605
1529.232261	201409.566641	36.675623
1530.520724	201759.119795	36.680640
1532.158302	202090.244857	36.685658
1534.007100	202422.682396	36.690676
1535.007859	202746.081779	36.695693
1536.793840	203051.374107	36.700711
1537.959858	203380.234029	36.705728
1539.253501	203701.671995	36.710746
1540.888167	204041.224451	36.715764
1542.195081	204363.894692	36.720781
1543.962215	204702.183941	36.725799
1545.306385	205045.382216	36.730816
1547.046170	205371.768999	36.735834
1548.089461	205721.787656	36.740852
1549.993976	206076.338242	36.745869
1551.624728	206410.746777	36.750887
1552.616881	206765.070311	36.755904
1554.071089	207107.370722	36.760922
1555.792828	207459.151602	36.765940
1557.204832	207825.803359	36.770957
1558.929871	208178.818529	36.775975
1560.113970	208534.502254	36.780992
1562.205390	208898.316604	36.786010
1563.174365	209259.118147	36.791028
1565.060172	209637.394512	36.796045
1566.792585	209996.663660	36.801063
1568.161548	210371.333622	36.806080
1569.806634	210737.553485	36.811098
1571.533639	211104.320107	36.816116
1573.109438	211476.167159	36.821133
1574.599079	211856.639462	36.826151
1576.275568	212223.673135	36.831168
1577.864037	212594.430804	36.836186
1579.494508	212973.614833	36.841204
1580.801486	213360.320615	36.846221
1582.807916	213734.112385	36.851239
1584.063703	214114.861539	36.856256
1585.702181	214495.625240	36.861274
1587.251673	214869.395538	36.866292
1588.800973	215265.491738	36.871309
1590.589609	215644.355906	36.876327
1591.914854	216030.307898	36.881344
1593.639306	216413.554124	36.886362
1594.792852	216807.995057	36.891380
1597.040870	217201.672617	36.896397
1598.852980	217586.255057	36.901415
1600.067487	217975.458586	36.906432
1601.874519	218371.296278	36.911450
1604.054744	218761.765601	36.916468
1605.534024	219150.498124	36.921485
1607.139843	219541.014501	36.926503
1608.726346	219924.728687	36.931520
1610.239419	220302.182909	36.936538
1612.334160	220687.517611	36.941556
1613.675538	221075.289452	36.946573
1615.562469	221460.762834	36.951591
1617.068522	221842.871611	36.956608
1618.617444	222228.124120	36.961626
1620.251040	222608.741295	36.966644
1621.732542	223004.141905	36.971661
1623.183299	223404.476453	36.976679
1624.708622	223858.774107	36.981696
1626.368975	224258.746764	36.986714
1627.941743	224634.453101	36.991732
1629.593331	225029.756238	36.996749
1631.400174	225421.936227	37.001767
1632.752809	225815.665698	37.006784
1634.170211	226219.088533	37.011802
1635.936619	226605.030517	37.016820
1637.574813	227007.530382	37.021837
1639.124411	227392.900946	37.026855
1640.672098	227779.746181	37.031872
1642.241956	228160.848388	37.036890
1644.111004	228541.241840	37.041908
1645.995761	228919.627118	37.046925
1647.791507	229283.752984	37.051943
1649.245137	229667.063048	37.056960
1650.376421	230049.868584	37.061978
1651.961799	230436.765871	37.066996
1653.432911	230826.883580	37.072013
1655.191942	231212.661999	37.077031
1656.829040	231594.702204	37.082048
1658.146234	231996.101060	37.087066
1659.941918	232398.590378	37.092084
1661.283778	232816.142434	37.097101
1663.205923	233210.890968	37.102119
1664.999368	233619.276863	37.107136
1666.691845	234030.576222	37.112154
1668.592178	234436.380942	37.117172
1669.601995	234849.547780	37.122189
1671.777196	235260.033747	37.127207
1673.264687	235677.264115	37.132224
1674.788989	236102.871951	37.137242
1676.520415	236515.313845	37.142260
1678.033443	236935.057664	37.147277
1679.781717	237365.533967	37.152295
1681.403534	237793.085494	37.157312
1683.088035	238230.610592	37.162330
1684.910020	238656.555992	37.167348
1686.730451	239086.160441	37.172365
1688.378494	239515.819650	37.177383
1689.972042	239948.740209	37.182400
1691.976137	240378.443927	37.187418
1693.980459	240809.088319	37.192436
1695.418774	241244.247025	37.197453
1697.272071	241680.938341	37.202471
1699.098473	242110.547603	37.207488
1700.600643	242544.986839	37.212506
1702.813592	242974.457524	37.217524
1704.393105	243418.157386	37.222541
1706.281372	243845.650908	37.227559
1707.692113	244277.999669	37.232576
1709.718015	244721.653291	37.237594
1711.555732	245146.642246	37.242612
1713.129767	245574.698281	37.247629
1715.067086	246006.937165	37.252647
1716.622962	246442.897641	37.257664
1718.201756	246878.854897	37.262682
1720.331153	247312.562506	37.267700
1721.714019	247738.900077	37.272717
1723.430932	248187.969418	37.277735
1725.342170	248615.567046	37.282752
1727.007152	249052.909752	37.287770
1728.926817	249492.420904	37.292788
1730.295470	249933.623893	37.297805
1732.857208	250373.004432	37.302823
1734.339168	250818.304815	37.307840
1735.776029	251243.239709	37.312858
1737.637253	251672.829822	37.317876
1739.604703	252108.550272	37.322893
1741.063585	252554.516302	37.327911
1743.178273	252984.751334	37.332928
1744.729659	253420.439742	37.337946
1746.671366	253850.830855	37.342964
1748.133989	254282.215830	37.347981
1749.796042	254724.643885	37.352999
1751.681531	255150.040434	37.358016
1752.972258	255593.292262	37.363034
1754.946084	256023.450332	37.368052
1756.790419	256440.115355	37.373069
1758.093867	256862.941195	37.378087
1760.041760	257277.861858	37.383104
1761.709920	257703.726796	37.388122
1763.462847	258119.111613	37.393140
1765.239004	258546.279747	37.398157
1767.023682	258976.444068	37.403175
1768.682568	259400.278322	37.408192
1770.186834	259832.470361	37.413210
1771.980362	260263.725454	37.418228
1773.369572	260697.689193	37.423245
1775.212491	261139.554531	37.428263
1777.023325	261581.526660	37.433280
1778.783086	262032.677664	37.438298
1780.842112	262477.072609	37.443316
1782.327872	262929.233829	37.448333
1784.234810	263372.561156	37.453351
1785.994729	263824.600436	37.458368
1787.596715	264289.697385	37.463386
1789.375670	264739.853132	37.468404
1791.237870	265211.409700	37.473421
1792.815254	265665.815016	37.478439
1794.537024	266133.100918	37.483456
1796.134219	266601.423116	37.488474
1798.581941	267060.230678	37.493492
1800.273036	267551.704083	37.498509
1802.193024	268006.762018	37.503527
1804.207940	268485.962055	37.508544
1805.914289	268962.570588	37.513562
1807.890060	269429.785768	37.518580
1810.069617	269906.086357	37.523597
1811.811898	270372.627625	37.528615
1813.811457	270841.945490	37.533632
1815.644988	271314.897315	37.538650
1817.172147	271785.638195	37.543668
1819.120565	272267.968640	37.548685
1820.782939	272729.312125	37.553703
1822.811221	273204.108651	37.558720
1824.621496	273686.510349	37.563738
1826.952145	274158.816644	37.568756
1828.674611	274633.305536	37.573773
1830.449290	275105.524103	37.578791
1832.550893	275575.630183	37.583808
1834.119891	276051.742054	37.588826
1836.580372	276516.173083	37.593844
1838.257907	276983.907750	37.598861
1839.785672	277457.330857	37.603879
1841.831785	277929.956067	37.608896
1843.386903	278407.538507	37.613914
1845.292837	278878.254162	37.618932
1847.172025	279360.759648	37.623949
1849.348717	279833.892321	37.628967
1851.306458	280308.457091	37.633984
1853.175033	280776.456329	37.639002
1855.038913	281242.981854	37.644020
1856.911231	281720.300480	37.649037
1858.481986	282203.357569	37.654055
1860.480196	282673.311749	37.659072
1862.193806	283150.906655	37.664090
1864.202088	283624.666725	37.669108
1866.331703	284092.867904	37.674125
1868.210553	284562.379187	37.679143
1870.177753	285040.714074	37.684160
1872.113615	285514.455064	37.689178
1874.111746	285982.570678	37.694196
1875.972540	286441.588581	37.699213
1877.583603	286920.509724	37.704231
1879.901101	287369.390559	37.709248
1881.383575	287825.215243	37.714266
1883.362920	288267.214681	37.719284
1885.204598	288710.276855	37.724301
1886.563130	289166.371571	37.729319
1888.604457	289595.478442	37.734336
1890.241518	290050.076309	37.739354
1892.369779	290498.114434	37.744372
1893.725144	290955.371842	37.749389
1895.557923	291415.596752	37.754407
1897.605893	291873.498437	37.759424
1899.218389	292349.758158	37.764442
1901.012073	292816.918404	37.769460
1902.836700	293293.393353	37.774477
1904.565226	293782.023185	37.779495
1906.357741	294249.330336	37.784512
1908.124382	294749.303287	37.789530
1910.101026	295230.164598	37.794548
1912.185542	295729.623507	37.799565
1913.541992	296228.006624	37.804583
1915.668651	296720.824930	37.809600
1917.919963	297235.133057	37.814618
1919.666213	297741.597736	37.819636
1921.485946	298240.707679	37.824653
1923.716533	298745.715962	37.829671
1925.417179	299247.482084	37.834688
1927.447542	299767.046078	37.839706
1929.481132	300281.324054	37.844724
1931.774528	300790.476876	37.849741
1933.689699	301307.816717	37.854759
1935.855353	301807.588123	37.859776
1937.941520	302321.389358	37.864794
1939.764730	302831.167631	37.869812
1941.833805	303343.010449	37.874829
1943.620800	303861.043033	37.879847
1945.681793	304371.789314	37.884864
1947.568912	304883.780421	37.889882
1949.405772	305403.040253	37.894900
1951.775443	305919.237645	37.899917
1953.667361	306443.967767	37.904935
1955.832540	306962.478306	37.909952
1957.825847	307472.328648	37.914970
1959.793713	307984.795839	37.919988
1961.847515	308499.709035	37.925005
1963.699760	309025.597688	37.930023
1965.886285	309531.848003	37.935040
1967.914896	310051.631376	37.940058
1969.882001	310565.352116	37.945076
1972.234922	311078.294740	37.950093
1973.929146	311600.408605	37.955111
1976.202279	312116.608027	37.960128
1978.460756	312620.058472	37.965146
1980.032252	313135.681171	37.970164
1982.439558	313637.271860	37.975181
1983.831921	314155.456469	37.980199
1985.950778	314662.420497	37.985216
1987.855629	315183.408069	37.990234
1989.734192	315702.517125	37.995252
1991.738010	316215.507414	38.000269
1993.789609	316741.664962	38.005287
1995.753514	317258.945633	38.010304
1997.802453	317790.758273	38.015322
1999.742346	318301.102998	38.020340
2001.943527	318814.854088	38.025357
2003.367028	319354.197696	38.030375
2006.160852	319869.442593	38.035392
2007.940295	320392.392240	38.040410
2009.508759	320905.038347	38.045428
2011.747377	321418.179182	38.050445
2013.641274	321927.107219	38.055463
2015.670147	322422.475739	38.060480
2017.803647	322921.149296	38.065498
2019.874901	323417.594869	38.070516
2022.045388	323905.996888	38.075533
2023.675190	324409.718265	38.080551
2026.051814	324897.240607	38.085568
2027.791226	325409.060423	38.090586
2029.742843	325917.337202	38.095604
2031.746507	326408.692048	38.100621
2033.577507	326914.644559	38.105639
2035.574394	327419.702185	38.110656
2037.446037	327944.045951	38.115674
2039.412791	328460.143587	38.120692
2041.403086	328978.949282	38.125709
2043.208146	329513.267397	38.130727
2045.335826	330048.517396	38.135744
2047.624071	330587.899369	38.140762
2049.060488	331122.567934	38.145780
2051.533654	331659.091191	38.150797
2053.609797	332210.881330	38.155815
2055.142435	332737.877218	38.160832
2057.494598	333300.273111	38.165850
2059.644468	333843.403477	38.170868
2061.851877	334392.382941	38.175885
2063.883303	334945.980576	38.180903
2066.080236	335503.835202	38.185920
2068.120989	336059.298202	38.190938
2070.138926	336618.059080	38.195956
2072.569222	337172.075232	38.200973
2074.322341	337739.396860	38.205991
2076.771446	338291.824113	38.211008
2078.709896	338859.255075	38.216026
2080.762200	339420.188242	38.221044
2083.263595	339977.512836	38.226061
2085.168618	340553.433472	38.231079
2087.162743	341115.804059	38.236096
2089.529108	341678.741340	38.241114
2091.207514	342249.171767	38.246132
2093.704385	342811.617596	38.251149
2095.595347	343384.690014	38.256167
2097.848987	343947.492708	38.261184
2100.327940	344517.891062	38.266202
2102.035715	345092.876756	38.271220
2104.503790	345650.725500	38.276237
2106.400458	346234.599706	38.281255
2108.762017	346807.578339	38.286272
2110.988912	347376.917552	38.291290
2112.915600	347946.045479	38.296308
2115.372800	348521.956212	38.301325
2117.499799	349089.488694	38.306343
2119.583633	349647.301559	38.311360
2122.062750	350220.217789	38.316378
2123.537593	350793.368555	38.321396
2125.898595	351361.823205	38.326413
2128.170419	351943.125585	38.331431
2130.569780	352512.929277	38.336448
2132.678699	353084.473591	38.341466
2134.386444	353659.984338	38.346484
2136.827876	354218.694959	38.351501
2138.699105	354794.975434	38.356519
2140.995665	355358.744507	38.361536
2142.871514	355943.458153	38.366554
2145.015251	356508.328091	38.371572
2147.018058	357085.697211	38.376589
2149.458294	357669.735227	38.381607
2151.347692	358242.742754	38.386624
2153.825254	358810.317027	38.391642
2155.876089	359361.309965	38.396660
2157.968985	359904.347208	38.401677
2160.150844	360456.800459	38.406695
2162.126496	361008.620478	38.411712
2164.382204	361544.986817	38.416730
2166.127867	362101.066452	38.421748
2168.463352	362655.011299	38.426765
2170.515896	363211.582675	38.431783
2172.667514	363767.673100	38.436800
2174.857970	364328.695994	38.441818
2176.871969	364901.815088	38.446836
2178.870429	365461.610088	38.451853
2180.968087	366034.393971	38.456871
2183.063848	366604.607442	38.461888
2185.474919	367200.355171	38.466906
2187.455396	367787.590726	38.471924
2189.695816	368372.059985	38.476941
2191.728096	368960.790415	38.481959
2193.590982	369554.840698	38.486976
2196.261667	370150.269904	38.491994
2197.974916	370756.018465	38.497012
2200.526825	371351.878808	38.502029
2202.495769	371960.076029	38.507047
2204.530488	372569.723142	38.512064
2207.179439	373182.809209	38.517082
2208.938416	373803.995266	38.522100
2211.008161	374425.271277	38.527117
2213.780712	375040.561883	38.532135
2215.902153	375665.383295	38.537152
2218.215078	376290.009711	38.542170
2220.188356	376909.329996	38.547188
2222.942496	377535.179740	38.552205
2224.860647	378165.010560	38.557223
2226.978508	378798.270858	38.562240
2229.558409	379423.227094	38.567258
2231.832996	380070.257709	38.572276
2234.430429	380703.529806	38.577293
2236.683952	381337.835529	38.582311
2238.908616	381963.563564	38.587328
2241.202766	382595.252149	38.592346
2243.275442	383227.953968	38.597364
2245.679110	383866.014752	38.602381
2247.607472	384499.222774	38.607399
2249.948248	385135.722331	38.612416
2252.689131	385779.318139	38.617434
2254.567755	386425.172913	38.622452
2256.926140	387054.405920	38.627469
2259.165456	387707.172213	38.632487
2261.198675	388342.948528	38.637504
2264.376117	388985.849365	38.642522
2266.256142	389634.604097	38.647540
2268.956496	390275.199483	38.652557
2271.190255	390915.351607	38.657575
2273.259477	391554.883842	38.662592
2275.646481	392190.142525	38.667610
2278.131828	392840.123802	38.672628
2280.436622	393469.057827	38.677645
2282.604464	394102.360868	38.682663
2285.203953	394738.494047	38.687680
2287.464399	395362.301220	38.692698
2289.484790	396008.387433	38.697716
2291.825481	396645.865745	38.702733
2294.453348	397286.146666	38.707751
2296.501249	397916.093379	38.712768
2298.985359	398549.527768	38.717786
2301.241502	399183.112666	38.722804
2303.511062	399811.055703	38.727821
2306.020119	400437.197002	38.732839
2307.985078	401042.078007	38.737856
2310.229753	401645.328963	38.742874
2312.324393	402256.320281	38.747892
2314.773286	402855.026763	38.752909
2316.725983	403459.199392	38.757927
2319.296722	404066.702897	38.762944
2321.731602	404675.507782	38.767962
2323.752847	405294.654141	38.772980
2326.059940	405906.721476	38.777997
2328.402547	406526.724607	38.783015
2330.537949	407155.209686	38.788032
2332.587959	407774.067476	38.793050
2334.613379	408416.728687	38.798068
2336.563404	409056.600489	38.803085
2339.389188	409702.139005	38.808103
2341.534182	410355.652484	38.813120
2343.743170	411006.049055	38.818138
2346.144106	411671.064346	38.823156
2347.947488	412328.891938	38.828173
2350.440230	412989.147618	38.833191
2352.678987	413671.641669	38.838208
2355.359633	414329.527705	38.843226
2357.677509	415023.750778	38.848244
2359.945428	415700.007063	38.853261
2362.254516	416381.304005	38.858279
2364.476379	417068.751290	38.863296
2366.972073	417752.083019	38.868314
2368.995307	418454.897702	38.873332
2371.870621	419149.879432	38.878349
2374.030789	419855.595432	38.883367
2376.181273	420562.533988	38.888384
2379.384089	421258.492227	38.893402
2381.550797	421968.477475	38.898420
2383.752754	422678.082126	38.903437
2386.483278	423378.666982	38.908455
2388.622868	424096.191199	38.913472
2391.111350	424803.256748	38.918490
2393.311131	425525.944421	38.923508
2396.030989	426239.259195	38.928525
2398.587320	426951.466046	38.933543
2400.699214	427676.635442	38.938560
2402.895647	428382.075041	38.943578
2405.489217	429116.031673	38.948596
2408.006286	429852.408207	38.953613
2411.078594	430572.572295	38.958631
2413.044946	431298.060179	38.963648
2415.558912	432025.358799	38.968666
2418.028902	432744.290116	38.973684
2420.785221	433470.491298	38.978701
2423.445987	434192.383243	38.983719
2425.401269	434917.861294	38.988736
2427.809033	435633.625620	38.993754
2430.472698	436368.000312	38.998772
2432.652784	437085.528017	39.003789
2435.711804	437814.679312	39.008807
2437.860717	438538.795544	39.013824
2440.441986	439262.715925	39.018842
2442.857376	440000.505116	39.023860
2444.997100	440725.614826	39.028877
2447.858470	441446.230355	39.033895
2450.195768	442170.501250	39.038912
2452.752660	442905.337052	39.043930
2455.430495	443628.694232	39.048948
2457.769205	444364.781917	39.053965
2460.124233	445084.299152	39.058983
2462.415928	445809.215909	39.064000
2465.035939	446533.244791	39.069018
2467.907499	447256.853717	39.074036
2470.056307	447948.588945	39.079053
2472.903683	448627.591714	39.084071
2475.025200	449316.454497	39.089088
2477.086374	450010.210946	39.094106
2479.585817	450707.918427	39.099124
2482.075511	451397.158376	39.104141
2484.396735	452088.426394	39.109159
2486.733093	452797.773652	39.114176
2489.518163	453491.902330	39.119194
2491.835618	454207.525798	39.124212
2494.035103	454910.957457	39.129229
2496.495971	455620.642531	39.134247
2498.616921	456348.005559	39.139264
2501.395333	457065.374823	39.144282
2503.980816	457800.446364	39.149300
2506.145015	458535.307980	39.154317
2508.768763	459267.741495	39.159335
2511.283203	460015.484154	39.164352
2513.776256	460761.382594	39.169370
2516.539500	461510.292148	39.174388
2518.138069	462255.978955	39.179405
2520.805059	463002.573467	39.184423
2523.391487	463780.490399	39.189440
2526.047075	464543.707957	39.194458
2528.351145	465313.119687	39.199476
2530.804282	466085.660409	39.204493
2533.495113	466863.538599	39.209511
2535.665952	467652.386704	39.214528
2538.804788	468451.705117	39.219546
2541.126801	469239.604247	39.224564
2543.747936	470025.602620	39.229581
2546.578139	470812.746737	39.234599
2549.141203	471608.036626	39.239616
2551.772702	472403.989123	39.244634
2554.332980	473200.576532	39.249652
2556.883774	474000.112251	39.254669
2559.795835	474788.491429	39.259687
2561.930077	475600.100490	39.264704
2564.939747	476387.789666	39.269722
2567.285142	477195.051188	39.274740
2570.111522	478003.309158	39.279757
2572.761096	478792.419684	39.284775
2575.632960	479595.903055	39.289792
2577.765569	480393.867508	39.294810
2580.561855	481205.624715	39.299828
2583.152222	482001.675483	39.304845
2586.184390	482811.857227	39.309863
2588.639593	483616.897070	39.314880
2591.220441	484414.003790	39.319898
2594.005169	485232.194921	39.324916
2596.514036	486027.575211	39.329933
2599.252565	486834.946961	39.334951
2602.032436	487639.044263	39.339968
2604.679483	488447.518170	39.344986
2607.384224	489236.361098	39.350004
2609.984281	490051.885461	39.355021
2612.354138	490847.928166	39.360039
2615.016735	491655.342143	39.365056
2617.895883	492449.309347	39.370074
2620.716755	493250.667558	39.375092
2623.066462	494050.804511	39.380109
2625.908561	494850.620928	39.385127
2628.960847	495650.062349	39.390144
2631.239670	496449.442314	39.395162
2633.707981	497249.661339	39.400180
2636.377479	498051.473965	39.405197
2638.923227	498844.188387	39.410215
2641.282296	499635.332279	39.415232
2644.050630	500408.161751	39.420250
2647.015058	501171.541246	39.425268
2649.323263	501948.914360	39.430285
2651.957123	502697.449504	39.435303
2654.264728	503471.976984	39.440320
2656.751966	504241.899583	39.445338
2659.149072	505023.046095	39.450356
2661.827611	505804.310438	39.455373
2664.665720	506591.309465	39.460391
2666.813561	507388.518511	39.465408
2669.245857	508178.683634	39.470426
2672.123790	508975.744118	39.475444
2674.503853	509782.324636	39.480461
2677.184780	510593.654160	39.485479
2679.568302	511414.417569	39.490496
2682.112639	512230.777198	39.495514
2684.778937	513062.396811	39.500532
2687.643599	513898.374974	39.505549
2690.295599	514724.113186	39.510567
2692.847256	515577.339543	39.515584
2695.695718	516414.949778	39.520602
2698.308508	517273.112284	39.525620
2701.099516	518124.043099	39.530637
2703.369731	518987.810190	39.535655
2706.130159	519854.118097	39.540672
2709.029838	520715.366756	39.545690
2711.819113	521588.876439	39.550708
2713.939198	522467.584293	39.555725
2716.951453	523330.983571	39.560743
2720.275371	524226.365074	39.565760
2723.060003	525105.968471	39.570778
2725.905472	525990.093063	39.575796
2728.665416	526868.539595	39.580813
2731.691854	527744.171348	39.585831
2734.309595	528640.815206	39.590848
2736.672500	529509.956989	39.595866
2739.965228	530401.448720	39.600884
2742.501274	531299.404635	39.605901
2745.647088	532180.744291	39.610919
2748.209145	533070.583459	39.615936
2751.087488	533969.426288	39.620954
2754.204060	534854.031633	39.625972
2757.173980	535750.987342	39.630989
2759.697593	536637.644630	39.636007
2762.375860	537531.467803	39.641024
2765.229789	538432.904716	39.646042
2767.960344	539315.286483	39.651060
2770.927493	540215.283838	39.656077
2773.532661	541112.869025	39.661095
2776.457266	542003.251648	39.666112
2779.371746	542913.448551	39.671130
2782.502868	543794.830726	39.676148
2785.025991	544697.079612	39.681165
2788.021903	545591.849649	39.686183
2791.090737	546482.124726	39.691200
2793.736729	547385.436112	39.696218
2796.629724	548274.267182	39.701236
2799.125441	549159.586912	39.706253
2802.517863	550062.046545	39.711271
2805.230107	550951.437896	39.716288
2807.856937	551834.099625	39.721306
2811.093897	552714.240958	39.726324
2813.669143	553611.171465	39.731341
2816.555744	554496.230568	39.736359
2819.512907	555384.436197	39.741376
2821.801332	556269.678220	39.746394
2824.841350	557146.547212	39.751412
2827.931824	558028.977716	39.756429
2830.632178	558882.022401	39.761447
2833.370201	559731.439030	39.766464
2836.209949	560577.016628	39.771482
2838.962171	561417.581398	39.776500
2841.692526	562274.169354	39.781517
2844.183282	563115.421918	39.786535
2846.946751	563973.098604	39.791552
2849.562392	564826.273672	39.796570
2852.759893	565692.905284	39.801588
2855.194243	566567.538330	39.806605
2857.797271	567432.444142	39.811623
2860.702955	568311.600799	39.816640
2863.365281	569196.008605	39.821658
2866.392355	570082.052093	39.826676
2868.946744	570985.780738	39.831693
2871.464868	571876.551868	39.836711
2874.647425	572783.963909	39.841728
2877.126494	573701.463722	39.846746
2880.204317	574615.084621	39.851764
2882.973018	575543.191263	39.856781
2885.661470	576476.962138	39.861799
2888.468342	577407.282284	39.866816
2891.201847	578345.170216	39.871834
2894.342806	579280.612613	39.876852
2897.138585	580239.214307	39.881869
2900.134226	581192.693093	39.886887
2903.277779	582135.391474	39.891904
2905.732292	583099.042079	39.896922
2908.892944	584058.388543	39.901940
2911.514830	585033.291235	39.906957
2914.472704	586000.991261	39.911975
2917.622575	586975.199473	39.916992
2920.472776	587960.506489	39.922010
2923.326566	588934.304279	39.927028
2926.300183	589928.050506	39.932045
2929.200004	590917.667012	39.937063
2932.394159	591904.346607	39.942080
2935.177981	592901.283530	39.947098
2937.968772	593892.624170	39.952116
2940.773287	594906.923979	39.957133
2943.583034	595919.231920	39.962151
2946.880004	596920.603068	39.967168
2949.398957	597940.798273	39.972186
2952.425752	598945.445888	39.977204
2955.590379	599981.281020	39.982221
2958.423605	601007.364322	39.987239
2961.626650	602023.682618	39.992256
2964.251529	603063.535592	39.997274
2967.672249	604089.547389	40.002292
2970.385354	605133.903113	40.007309
2973.241121	606157.819916	40.012327
2976.292797	607195.574328	40.017344
2979.184933	608247.871346	40.022362
2982.245031	609281.029380	40.027380
2985.280189	610320.100205	40.032397
2988.562560	611372.590817	40.037415
2991.240762	612403.122850	40.042432
2994.226840	613452.414836	40.047450
2997.033655	614491.384918	40.052468
2999.803771	615552.766466	40.057485
3002.936822	616604.885781	40.062503
3006.245710	617656.675471	40.067520
3008.966721	618729.107897	40.072538
3012.142894	619779.715622	40.077556
3014.928054	620844.131603	40.082573
3018.139663	621900.376573	40.087591
3021.237630	622965.232445	40.092608
3024.067647	624018.335003	40.097626
3026.869303	625031.518785	40.102644
3029.944695	626064.145334	40.107661
3032.769961	627083.975312	40.112679
3035.922531	628102.355120	40.117696
3038.271370	629141.646345	40.122714
3041.450738	630172.408906	40.127732
3044.393985	631213.146551	40.132749
3047.082087	632256.769249	40.137767
3050.342187	633299.694711	40.142784
3052.945361	634368.233001	40.147802
3055.813773	635427.733545	40.152820
3059.092996	636497.888686	40.157837
3061.803080	637575.762304	40.162855
3064.661229	638654.197770	40.167872
3067.274908	639744.634860	40.172890
3070.651354	640844.658407	40.177908
3073.437461	641954.088924	40.182925
3076.451297	643062.314000	40.187943
3079.241788	644175.043454	40.192960
3082.421192	645318.703087	40.197978
3085.754881	646452.585018	40.202996
3088.639520	647585.765390	40.208013
3091.572633	648736.257160	40.213031
3094.816479	649872.908624	40.218048
3097.375387	651040.791718	40.223066
3101.008595	652195.055750	40.228084
3103.764706	653368.014758	40.233101
3106.754040	654537.358713	40.238119
3110.273875	655721.619959	40.243136
3113.224460	656895.472340	40.248154
3116.522344	658084.316387	40.253172
3119.436890	659268.149129	40.258189
3122.719108	660470.896504	40.263207
3126.144644	661658.287223	40.268224
3129.102847	662864.225885	40.273242
3131.998414	664054.993170	40.278260
3135.775206	665267.314392	40.283277
3138.468830	666476.476143	40.288295
3142.015336	667684.846641	40.293312
3144.600144	668910.384498	40.298330
3147.792848	670126.710723	40.303348
3151.422356	671340.868853	40.308365
3154.534394	672567.039356	40.313383
3158.103562	673784.323139	40.318400
3161.210098	675014.201828	40.323418
3164.469535	676236.834821	40.328436
3167.836485	677451.436694	40.333453
3170.758538	678668.288382	40.338471
3174.325186	679890.388896	40.343488
3177.176546	681108.271976	40.348506
3180.815085	682334.854807	40.353524
3184.185589	683563.900131	40.358541
3187.360536	684789.286199	40.363559
3190.623871	685996.617099	40.368576
3193.461740	687215.673453	40.373594
3197.011766	688445.368965	40.378612
3200.601011	689655.781048	40.383629
3203.277322	690883.897397	40.388647
3207.008263	692092.865285	40.393664
3210.302008	693303.329074	40.398682
3213.218487	694522.321971	40.403700
3216.825766	695738.603064	40.408717
3219.939292	696955.194949	40.413735
3223.456998	698153.651546	40.418752
3226.578113	699376.552029	40.423770
3229.489189	700598.126671	40.428788
3232.858744	701800.619844	40.433805
3236.260707	703007.154107	40.438823
3239.291865	704173.642624	40.443840
3242.614945	705346.763110	40.448858
3245.758399	706501.077509	40.453876
3249.065252	707646.343811	40.458893
3251.719732	708822.617378	40.463911
3254.846492	709985.974553	40.468928
3258.223599	711164.034936	40.473946
3261.384505	712341.274686	40.478964
3264.435361	713512.973823	40.483981
3267.635020	714707.846014	40.488999
3270.845367	715899.330609	40.494016
3273.942037	717106.052480	40.499034
3277.121508	718302.593993	40.504052
3280.567208	719496.991234	40.509069
3283.645709	720724.116463	40.514087
3286.891765	721923.588864	40.519104
3290.068773	723161.759836	40.524122
3293.078288	724386.722226	40.529140
3296.772184	725621.176026	40.534157
3299.828467	726866.619097	40.539175
3302.717714	728103.994338	40.544192
3306.250012	729355.946554	40.549210
3309.424553	730623.967005	40.554228
3312.815059	731895.803466	40.559245
3315.824421	733180.391013	40.564263
3319.390823	734444.340478	40.569280
3322.617944	735730.163824	40.574298
3325.642550	737027.807917	40.579316
3328.990057	738310.778095	40.584333
3331.987785	739620.095270	40.589351
3335.354275	740919.466511	40.594368
3338.724583	742242.151588	40.599386
3341.782473	743564.814330	40.604404
3345.403212	744886.816722	40.609421
3348.270047	746230.708002	40.614439
3351.853798	747561.187954	40.619456
3355.369410	748904.906053	40.624474
3358.346766	750263.311818	40.629492
3362.059826	751597.168739	40.634509
3365.389255	752967.899416	40.639527
3368.484657	754327.491401	40.644544
3371.797566	755689.662396	40.649562
3375.331092	757057.855812	40.654580
3379.138930	758417.144607	40.659597
3382.286670	759796.919045	40.664615
3385.480430	761166.987412	40.669632
3389.025572	762538.667825	40.674650
3392.239312	763929.187675	40.679668
3395.616105	765312.390662	40.684685
3399.355416	766701.866484	40.689703
3402.692603	768075.369730	40.694720
3406.218880	769469.525483	40.699738
3409.701619	770860.772446	40.704756
3413.259025	772244.522765	40.709773
3416.469227	773636.469906	40.714791
3419.810273	775025.332060	40.719808
3423.784618	776421.191553	40.724826
3426.958979	777809.895286	40.729844
3430.353233	779193.781775	40.734861
3433.925400	780591.213665	40.739879
3437.184510	781981.508640	40.744896
3440.938575	783375.868652	40.749914
3444.380192	784765.742307	40.754932
3447.887084	786150.971044	40.759949
3451.228669	787556.892536	40.764967
3454.622877	788940.861879	40.769984
3458.263918	790329.421195	40.775002
3461.245146	791707.549813	40.780007
3464.810988	793040.240858	40.785012
3468.092177	794329.268203	40.790016
3471.556331	795541.045300	40.795021
3474.746263	796698.218596	40.800026
3477.656478	797782.312223	40.805031
3480.972444	798800.019110	40.810036
3483.897952	799744.237335	40.815040
3486.173611	800603.657303	40.820045
3489.076007	801416.510284	40.825050
3491.287333	802168.118543	40.830055
3493.827247	802830.476520	40.835060
3495.918808	803458.957665	40.840064
3498.090332	804014.990615	40.845069
3500.072601	804511.631011	40.850074
3501.713673	804962.547032	40.855079
3503.926903	805344.799694	40.860084
3505.255402	805681.485995	40.865088
3506.945472	805962.553807	40.870093
3508.537298	806198.821314	40.875098
3510.125998	806403.267642	40.880103
3511.266084	806550.283493	40.885108
3512.440528	806649.498504	40.890112
3513.835345	806726.422050	40.895117
3515.190750	806773.255017	40.900122
3515.838266	806761.237328	40.905127
3516.963044	806728.995013	40.910132
3517.729598	806679.361399	40.915136
3518.432612	806582.288549	40.920141
3518.962731	806480.978173	40.925146
3519.708635	806345.709136	40.930151
3520.474234	806191.708226	40.935156
3521.133804	806011.200369	40.940160
3521.687518	805808.497520	40.945165
3521.692119	805589.847915	40.950170
3522.278806	805362.662808	40.955175
3522.877971	805114.287784	40.960180
3523.060594	804856.509516	40.965184
3523.513421	804588.478308	40.970189
3523.736223	804293.015270	40.975194
3524.191964	804005.543127	40.980199
3524.506112	803689.590800	40.985204
3524.993067	803368.544243	40.990208
3524.865809	803041.012081	40.995213
3525.417372	802696.873086	41.000218
3525.261229	802346.800550	41.005223
3525.406664	802004.263413	41.010228
3525.616764	801639.526506	41.015232
3525.708429	801271.650250	41.020237
3525.608226	800912.273145	41.025242
3524.798591	800543.378249	41.030247
3525.486134	800168.280267	41.035252
3525.491352	799789.300002	41.040256
3525.504648	799410.493950	41.045261
3525.996197	799024.669266	41.050266
3525.658485	798652.798806	41.055271
3525.415016	798260.623991	41.060276
3525.570669	797886.275499	41.065280
3525.626968	797492.290160	41.070285
3525.472838	797087.567456	41.075290
3525.389860	796692.627205	41.080295
3525.250145	796302.975781	41.085300
3525.346557	795920.725963	41.090304
3525.177341	795518.614886	41.095309
3525.358360	795121.185624	41.100314
3525.305152	794728.829913	41.105319
3524.875076	794322.175662	41.110324
3524.521071	793942.347241	41.115328
3525.012382	793543.156806	41.120333
3524.824120	793151.619095	41.125338
3524.480554	792757.285549	41.130343
3524.602776	792347.036902	41.135348
3524.282645	791958.352508	41.140352
3524.131082	791574.580445	41.145357
3524.298581	791188.818982	41.150362
3524.013810	790793.923718	41.155367
3524.013161	790381.714073	41.160372
3523.842960	790006.261507	41.165376
3523.516847	789630.569020	41.170381
3523.424141	789241.894226	41.175386
3523.135319	788857.063597	41.180391
3523.392455	788480.182040	41.185396
3523.111760	788099.044047	41.190400
3522.922558	787721.360256	41.195405
3522.738801	787339.674073	41.200410
3522.238257	786965.687985	41.205415
3522.266077	786601.476108	41.210420
3522.384044	786233.936977	41.215424
3522.328196	785871.078114	41.220429
3521.700088	785503.230982	41.225434
3521.263609	785148.461388	41.230439
3521.672759	784778.045950	41.235444
3521.354384	784422.335818	41.240448
3521.579806	784064.108798	41.245453
3521.404601	783709.323217	41.250458
3521.240109	783351.370747	41.255463
3521.016081	783003.935499	41.260468
3521.042959	782652.261325	41.265472
3520.712717	782308.007026	41.270477
3521.003708	781956.255328	41.275482
3520.630196	781601.791949	41.280487
3520.590913	781258.915370	41.285492
3520.376672	780901.882391	41.290496
3520.434209	780562.548220	41.295501
3520.366389	780225.678891	41.300506
3519.582064	779894.029205	41.305511
3519.951644	779553.513782	41.310516
3519.318662	779220.528922	41.315520
3519.670320	778900.309123	41.320525
3519.595907	778573.107859	41.325530
3519.215923	778241.857284	41.330535
3519.048540	777904.305878	41.335540
3518.729459	777593.785729	41.340544
3518.737336	777271.237427	41.345549
3518.835457	776954.025443	41.350554
3518.617958	776644.727915	41.355559
3518.514354	776326.488099	41.360564
3518.009949	776018.835846	41.365568
3517.826674	775704.717432	41.370573
3517.536979	775387.895119	41.375578
3517.213648	775101.788573	41.380583
3517.225806	774804.438315	41.385588
3517.500363	774514.812822	41.390592
3516.998555	774224.466671	41.395597
3517.230306	773924.582379	41.400602
3516.865948	773645.123003	41.405607
3516.816924	773347.723740	41.410612
3516.883688	773072.800933	41.415616
3516.567716	772796.453330	41.420621
3516.674796	772503.229891	41.425626
3516.289078	772221.848239	41.430631
3516.249401	771943.600599	41.435636
3516.205350	771672.633658	41.440640
3515.865810	771402.936990	41.445645
3515.840427	771115.443781	41.450650
3515.898164	770848.321628	41.455655
3515.726061	770577.384838	41.460660
3515.541709	770317.821289	41.465664
3515.400634	770059.965977	41.470669
3515.231491	769798.263050	41.475674
3515.250241	769528.488210	41.480679
3515.043555	769270.764047	41.485684
3514.781239	769012.744422	41.490688
3514.836687	768759.542127	41.495693
3514.536847	768500.574565	41.500698
3514.481334	768261.024408	41.505703
3514.184423	768008.396669	41.510708
3514.211426	767769.556342	41.515712
3514.150145	767523.724060	41.520717
3514.051241	767286.564755	41.525722
3513.805969	767053.020237	41.530727
3514.013375	766798.838913	41.535732
3513.703583	766557.895648	41.540736
3513.725736	766334.241926	41.545741
3513.689453	766100.830331	41.550746
3512.977709	765872.255391	41.555751
3513.517391	765643.023562	41.560756
3513.223072	765422.401981	41.565760
3513.291834	765200.629402	41.570765
3512.921466	764966.892322	41.575770
3512.965012	764748.709734	41.580775
3513.029375	764525.438704	41.585780
3512.714162	764311.986709	41.590784
3512.507566	764088.106283	41.595789
3512.579273	763874.282217	41.600794
3512.386607	763656.402634	41.605799
3512.285463	763442.890639	41.610804
3512.467331	763239.485014	41.615808
3512.434412	763020.574354	41.620813
3512.407860	762822.715328	41.625818
3511.883421	762615.710314	41.630823
3511.968503	762396.318167	41.635828
3511.709301	762197.938515	41.640832
3511.592795	761998.888914	41.645837
3511.386947	761796.741285	41.650842
3511.277529	761607.199948	41.655847
3511.534199	761414.880502	41.660852
3511.425012	761223.356375	41.665856
3511.264805	761027.494730	41.670861
3511.049716	760839.678094	41.675866
3511.043810	760660.504883	41.680871
3511.074315	760467.310596	41.685876
3510.709565	760274.719186	41.690880
3510.525243	760097.436773	41.695885
3510.683446	759901.148136	41.700890
3510.554510	759727.794953	41.705895
3510.433235	759541.854855	41.710900
3510.547817	759368.552012	41.715904
3510.118289	759199.331582	41.720909
3510.238537	759014.177567	41.725914
3510.157757	758852.441477	41.730919
3510.182481	758666.702595	41.735924
3510.016664	758503.838140	41.740928
3510.190415	758333.956203	41.745933
3510.031972	758156.328067	41.750938
3509.959758	757984.554240	41.755943
3509.941024	757817.308033	41.760948
3509.629936	757652.820697	41.765952
3509.617029	757478.706123	41.770957
3509.707940	757318.735197	41.775962
3509.543092	757171.388686	41.780967
3509.690996	757009.970583	41.785972
3509.539452	756851.609209	41.790976
3509.254541	756684.036480	41.795981
3509.401575	756517.079934	41.800986
3508.838781	756372.794497	41.805991
3509.222150	756227.215120	41.810996
3509.285353	756081.142738	41.816000
3509.063132	755916.553941	41.821005
3509.071905	755763.474836	41.826010
3508.710241	755607.047485	41.831015
3508.899486	755462.670312	41.836020
3508.719270	755299.097998	41.841024
3508.600255	755158.073491	41.846029
3508.788052	755011.318363	41.851034
3508.324675	754879.034454	41.856039
3508.528167	754747.033350	41.861044
3508.544136	754599.706199	41.866048
3508.407124	754455.906902	41.871053
3508.404191	754311.095339	41.876058
3508.213131	754176.038865	41.881063
3508.157967	754036.563195	41.886068
3508.205995	753887.686446	41.891072
3507.998225	753756.723602	41.896077
3507.962795	753628.495310	41.901082
3507.881080	753493.655708	41.906087
3508.159836	753359.297527	41.911092
3507.963753	753234.792634	41.916096
3507.512706	753101.142759	41.921101
3507.685501	752966.992712	41.926106
3507.474053	752846.829728	41.931111
3507.651260	752706.649660	41.936116
3507.603776	752587.542065	41.941120
3507.556418	752463.345881	41.946125
3507.840351	752334.203844	41.951130
3507.504589	752222.793018	41.956135
3507.149846	752088.220719	41.961140
3507.301084	751958.649764	41.966144
3507.276038	751845.058559	41.971149
3507.382321	751720.578149	41.976154
3506.943928	751610.212581	41.981159
3506.975504	751491.815903	41.986164
3507.013608	751370.057631	41.991168
3506.871324	751256.131329	41.996173
3507.159126	751129.289990	42.001178
3506.732771	751030.077238	42.006183
3506.992885	750907.632968	42.011188
3507.015549	750804.045907	42.016192
3506.350892	750694.939449	42.021197
3506.628513	750589.726805	42.026202
3506.739695	750478.068967	42.031207
3506.558939	750361.369511	42.036212
3506.509151	750263.715051	42.041216
3506.716522	750152.283667	42.046221
3506.674212	750045.584933	42.051226
3506.227936	749947.497803	42.056231
3506.499658	749842.078373	42.061236
3506.736024	749736.021095	42.066240
3506.220075	749634.433858	42.071245
3506.591886	749517.778864	42.076250
3506.158845	749416.619753	42.081255
3506.156341	749310.348990	42.086260
3506.310315	749218.428273	42.091264
3506.230119	749119.825695	42.096269
3506.384447	749013.327398	42.101274
3505.916075	748925.211333	42.106279
3506.142982	748816.178551	42.111284
3506.307222	748716.542400	42.116288
3506.155783	748625.307315	42.121293
3505.908825	748517.484857	42.126298
3506.121368	748433.154477	42.131303
3505.631035	748336.190699	42.136308
3505.909456	748250.661597	42.141312
3505.513591	748152.938779	42.146317
3505.837401	748059.049259	42.151322
3505.556899	747977.562353	42.156327
3505.588982	747874.725267	42.161332
3505.377857	747789.024683	42.166336
3505.421603	747697.252399	42.171341
3505.400995	747615.471801	42.176346
3505.322850	747539.234541	42.181351
3505.601768	747448.705427	42.186356
3505.566339	747371.421717	42.191360
3505.326404	747272.229026	42.196365
3505.418751	747183.556071	42.201370
3505.003346	747108.259715	42.206375
3505.516704	747018.774222	42.211380
3505.378971	746936.165652	42.216384
3505.161589	746858.313787	42.221389
3505.229166	746770.925183	42.226394
3504.762050	746698.549286	42.231399
3505.238634	746621.025514	42.236404
3505.354546	746533.873408	42.241408
3504.996471	746463.800271	42.246413
3505.251882	746382.109540	42.251418
3505.100312	746298.260891	42.256423
3505.357655	746221.807210	42.261428
3505.260803	746141.259365	42.266432
3505.066740	746055.833487	42.271437
3505.273632	745965.694469	42.276442
3504.949362	745885.873443	42.281447
3504.918226	745804.372176	42.286452
3504.970074	745744.407222	42.291456
3504.878814	745670.081586	42.296461
3505.022771	745579.948496	42.301466
3504.752051	745513.361938	42.306471
3504.798767	745441.581753	42.311476
3504.927722	745362.422165	42.316480
3504.790197	745301.051524	42.321485
3504.703425	745210.457889	42.326490
3504.970553	745149.217112	42.331495
3505.053388	745062.548397	42.336500
3504.874220	744989.170007	42.341504
3504.586023	744917.390772	42.346509
3504.320759	744845.804837	42.351514
3504.301131	744785.399414	42.356519
3504.466743	744713.395234	42.361524
3504.707495	744656.851280	42.366528
3504.640568	744585.823516	42.371533
3504.823199	744508.277845	42.376538
3504.587788	744438.809035	42.381543
3504.790303	744350.728512	42.386548
3504.595529	744288.914448	42.391552
3504.500272	744233.708190	42.396557
3504.998822	744148.691217	42.401562
3504.365746	744080.916233	42.406567
3504.684751	744017.482771	42.411572
3504.648779	743944.614852	42.416576
3504.145187	743880.821427	42.421581
3504.487515	743801.314300	42.426586
3504.240281	743746.821832	42.431591
3504.521785	743672.613616	42.436596
3504.264295	743612.436132	42.441600
3504.266356	743548.556693	42.446605
3504.480742	743483.306799	42.451610
3504.315445	743441.159375	42.456615
3504.293274	743359.136806	42.461620
3504.491942	743300.068414	42.466624
3504.380362	743229.431301	42.471629
3504.324118	743162.789459	42.476634
3504.162725	743111.789020	42.481639
3504.001064	743043.235179	42.486644
3504.535207	742983.960806	42.491648
3504.088653	742915.057224	42.496653
3504.426780	742853.341854	42.501658
3504.399981	742781.598929	42.506663
3504.507556	742720.464425	42.511668
3504.246039	742670.961054	42.516672
3504.173150	742604.069990	42.521677
3504.359073	742531.004081	42.526682
3504.017902	742485.616908	42.531687
3503.746119	742418.361448	42.536692
3504.184503	742346.785166	42.541696
3504.170008	742303.420010	42.546701
3504.118692	742230.291507	42.551706
3504.154570	742172.972267	42.556711
3504.241576	742116.880467	42.561716
3503.868470	742056.858500	42.566720
3504.027636	741999.517687	42.571725
3504.134646	741934.668289	42.576730
3503.932735	741873.874937	42.581735
3503.955726	741830.204288	42.586740
3503.881326	741759.399521	42.591744
3503.634797	741709.393109	42.596749
3504.214709	741650.645186	42.601754
3503.912369	741598.669101	42.606759
3503.742382	741544.692674	42.611764
3504.077400	741486.379521	42.616768
3503.610642	741439.276088	42.621773
3504.072203	741367.192565	42.626778
3503.885406	741318.113498	42.631783
3503.769603	741261.059917	42.636788
3503.814388	741205.265345	42.641792
3503.493267	741151.706792	42.646797
3503.998130	741099.891169	42.651802
3503.724968	741042.565194	42.656807
3503.742896	740982.074964	42.661812
3503.806017	740930.825605	42.666816
3503.492227	740887.056864	42.671821
3503.541110	740834.523295	42.676826
3503.528090	740788.923919	42.681831
3503.590132	740727.880424	42.686836
3503.655156	740680.932148	42.691840
3503.465848	740635.657698	42.696845
3503.766625	740571.754414	42.701850
3503.484005	740527.780706	42.706855
3503.472494	740475.650398	42.711860
3503.873922	740429.040894	42.716864
3503.573209	740373.297389	42.721869
3503.696577	740316.642754	42.726874
3503.876634	740281.197915	42.731879
3503.817941	740227.738257	42.736884
3503.483823	740185.057171	42.741888
3503.079309	740131.159209	42.746893
3503.611697	740074.534378	42.751898
3503.626765	740030.459395	42.756903
3503.437447	739980.630487	42.761908
3503.430255	739925.874229	42.766912
3503.361083	739886.659891	42.771917
3503.622597	739830.325278	42.776922
3503.621337	739784.866587	42.781927
3503.503676	739736.508313	42.786932
3503.375434	739682.957512	42.791937
3502.972598	739650.029755	42.796941
3503.270968	739588.790154	42.801946
3503.402205	739553.844784	42.806951
3503.157609	739510.057033	42.811956
3503.114465	739457.529507	42.816961
3503.024180	739425.489208	42.821965
3503.172848	739374.908254	42.826970
3502.912703	739342.598798	42.831975
3502.896691	739307.082982	42.836980
3502.870249	739264.840935	42.841985
3503.075147	739226.369683	42.846989
3503.552622	739177.514192	42.851994
3503.541849	739132.102803	42.856999
3503.284244	739083.862553	42.862004
3503.278794	739033.651114	42.867009
3503.448162	739006.562863	42.872013
3503.432621	738945.518446	42.877018
3503.673390	738909.513305	42.882023
3503.285656	738851.745126	42.887028
3503.538083	738801.341316	42.892033
3503.441621	738763.313257	42.897037
3503.540072	738719.266736	42.902042
3503.274318	738668.353794	42.907047
3503.146010	738615.884214	42.912052
3503.277471	738571.781964	42.917057
3503.169514	738531.577863	42.922061
3503.502055	738492.686247	42.927066
3503.447701	738454.204508	42.932071
3503.420008	738407.653868	42.937076
3503.362219	738354.131981	42.942081
3503.136002	738307.316616	42.947085
3503.216552	738261.984165	42.952090
3503.108441	738212.872920	42.957095
3502.990747	738178.605712	42.962100
3502.927362	738127.359110	42.967105
3503.065323	738104.428962	42.972109
3503.277408	738058.331535	42.977114
3503.004735	738008.108182	42.982119
3503.079029	737971.928330	42.987124
3502.996534	737926.126062	42.992129
3502.572519	737893.293465	42.997133
3502.994382	737855.225144	43.002138
3503.119765	737821.312170	43.007143
3502.986326	737777.595520	43.012148
3503.220200	737736.687866	43.017153
3502.731081	737707.477164	43.022157
3503.047674	737668.584160	43.027162
3503.034646	737627.568192	43.032167
3502.831016	737595.836078	43.037172
3503.101390	737530.973274	43.042177
3502.712852	737514.263679	43.047181
3503.019943	737470.175879	43.052186
3503.099921	737428.648762	43.057191
3502.916108	737392.360369	43.062196
3502.817823	737350.565334	43.067201
3502.805259	737320.928325	43.072205
3502.850074	737284.354364	43.077210
3502.722985	737248.649747	43.082215
3502.837985	737205.977625	43.087220
3503.148909	737173.713712	43.092225
3502.887532	737136.744188	43.097229
3503.050048	737089.016418	43.102234
3502.845695	737054.461763	43.107239
3503.028392	737012.074348	43.112244
3503.282730	736976.404633	43.117249
3503.058280	736949.770156	43.122253
3503.125036	736900.523053	43.127258
3502.746762	736870.548761	43.132263
3503.112681	736831.693043	43.137268
3502.996292	736794.797014	43.142273
3502.968317	736755.857377	43.147277
3502.890732	736716.331906	43.152282
3502.782526	736686.955729	43.157287
3502.551966	736644.436518	43.162292
3502.462271	736610.850757	43.167297
3502.821956	736591.888064	43.172301
3502.801998	736540.475662	43.177306
3502.661273	736516.943562	43.182311
3503.019734	736473.386152	43.187316
3502.964224	736442.862209	43.192321
3502.913457	736399.272852	43.197325
3503.176910	736351.425078	43.202330
3502.827833	736318.029287	43.207335
3503.197743	736285.207716	43.212340
3503.085930	736238.113923	43.217345
3502.759196	736209.068924	43.222349
3503.006100	736157.560605	43.227354
3503.087726	736129.536776	43.232359
3503.136347	736086.869623	43.237364
3503.335002	736050.017227	43.242369
3502.801653	736018.927043	43.247373
3502.991958	735969.257939	43.252378
3503.042170	735934.953436	43.257383
3502.811782	735897.725625	43.262388
3502.687057	735860.727682	43.267393
3502.861205	735831.945215	43.272397
3502.840427	735782.755149	43.277402
3502.976368	735753.087862	43.282407
3503.033315	735719.028780	43.287412
3503.083451	735678.635792	43.292417
3502.941831	735638.175213	43.297421
3503.160994	735602.901112	43.302426
3502.804309	735557.526385	43.307431
3502.883090	735521.730645	43.312436
3502.991532	735480.832131	43.317441
3502.741542	735454.691807	43.322445
3502.895597	735417.497404	43.327450
3502.778324	735386.187724	43.332455
3502.769794	735334.765702	43.337460
3502.977776	735302.065779	43.342465
3502.884715	735268.029499	43.347469
3503.293651	735233.217444	43.352474
3502.983607	735209.907376	43.357479
3503.240046	735173.338397	43.362484
3503.086092	735122.829878	43.367489
3502.646794	735084.098372	43.372493
3502.899379	735046.836523	43.377498
3502.935852	735014.411165	43.382503
3502.717277	734975.939740	43.387508
3502.829400	734945.134993	43.392513
3502.565132	734909.937504	43.397517
3502.982454	734874.825539	43.402522
3502.732429	734843.189140	43.407527
3502.409695	734805.476506	43.412532
3502.806974	734763.833796	43.417537
3502.503939	734744.926446	43.422541
3502.769492	734699.444335	43.427546
3502.467707	734671.132107	43.432551
3502.764880	734639.454240	43.437556
3502.897878	734608.694262	43.442561
3503.190325	734571.770130	43.447565
3502.970727	734528.643905	43.452570
3502.779118	734496.006544	43.457575
3502.784954	734465.266970	43.462580
3502.942659	734419.603053	43.467585
3502.792182	734393.541870	43.472589
3503.029049	734355.932916	43.477594
3502.864500	734323.438894	43.482599
3502.553807	734297.849297	43.487604
3502.631255	734255.910159	43.492609
3502.254522	734222.955691	43.497613
3502.549499	734195.582962	43.502618
3502.567528	734168.899281	43.507623
3502.725685	734138.875871	43.512628
3502.777637	734095.405573	43.517633
3502.834710	734068.665625	43.522637
3502.894032	734034.599010	43.527642
3502.859390	733999.557701	43.532647
3502.662524	733971.621732	43.537652
3503.172508	733931.292695	43.542657
3502.612464	733900.495697	43.547661
3502.763867	733856.215686	43.552666
3502.799168	733820.667048	43.557671
3502.541104	733797.294807	43.562676
3502.845947	733763.137087	43.567681
3502.802455	733733.343403	43.572685
3502.961735	733689.209686	43.577690
3502.773301	733646.865653	43.582695
3502.375311	733615.100287	43.587700
3502.868614	733589.920504	43.592705
3502.419151	733560.391089	43.597709
3502.591788	733530.957080	43.602714
3502.716058	733495.788386	43.607719
3502.243525	733470.519848	43.612724
3502.892237	733431.254563	43.617729
3502.619051	733414.467881	43.622733
3502.598870	733367.639185	43.627738
3502.203352	733332.456412	43.632743
3502.107715	733319.303701	43.637748
3502.694212	733277.325098	43.642753
3502.377028	733255.693737	43.647757
3502.576838	733221.006460	43.652762
3502.289654	733198.330367	43.657767
3502.370969	733176.979680	43.662772
3502.654539	733147.625008	43.667777
3502.641190	733116.239856	43.672781
3502.351091	733081.979253	43.677786
3502.476568	733066.858913	43.682791
3502.325263	733033.565382	43.687796
3502.513001	733003.780409	43.692801
3502.227119	732975.212048	43.697805
3502.779025	732939.277355	43.702810
3502.877604	732916.586415	43.707815
3502.976285	732871.864111	43.712820
3502.615957	732837.564532	43.717825
3502.446862	732816.204642	43.722829
3502.714246	732777.741649	43.727834
3502.524566	732755.246279	43.732839
3502.169618	732726.836945	43.737844
3502.953376	732686.704133	43.742849
3502.342262	732659.822062	43.747853
3502.679681	732632.139981	43.752858
3502.988102	732604.314052	43.757863
3502.603476	732563.729512	43.762868
3502.656488	732526.488897	43.767873
3502.822119	732499.181241	43.772877
3502.451807	732464.337100	43.777882
3502.399518	732440.035814	43.782887
3502.580086	732397.277839	43.787892
3502.521896	732379.958460	43.792897
3502.495281	732354.959526	43.797901
3502.599278	732326.671208	43.802906
3502.904621	732290.774263	43.807911
3502.512367	732263.706271	43.812916
3502.320063	732228.534707	43.817921
3502.371042	732184.905736	43.822925
3502.579252	732164.917823	43.827930
3502.759981	732142.161660	43.832935
3502.538400	732114.124297	43.837940
3502.546799	732076.888960	43.842945
3502.313070	732050.932943	43.847949
3502.266306	732016.627721	43.852954
3502.505694	731988.910079	43.857959
3502.468722	731962.624274	43.862964
3502.631195	731918.876469	43.867969
3502.616074	731909.768374	43.872973
3502.538713	731884.924891	43.877978
3502.551750	731847.192587	43.882983
3502.514296	731820.658826	43.887988
3502.765705	731786.154951	43.892993
3502.505990	731757.776028	43.897997
3502.555740	731731.029543	43.903002
3502.659011	731694.371001	43.908007
3502.553455	731659.677826	43.913012
3502.548978	731619.422030	43.918017
3502.475917	731603.737474	43.923021
3502.394675	731571.713797	43.928026
3502.670738	731551.118992	43.933031
3502.301357	731516.171572	43.938036
3502.485590	731478.310307	43.943041
3502.490705	731464.989421	43.948045
3502.331724	731420.796720	43.953050
3502.446725	731397.058945	43.958055
3502.340473	731381.379426	43.963060
3502.542517	731340.692075	43.968065
3502.561554	731309.542160	43.973069
3502.700004	731282.928135	43.978074
3502.672197	731256.143343	43.983079
3502.452441	731219.139728	43.988084
3502.608611	731190.492214	43.993089
3502.674932	731162.800264	43.998093
3502.583185	731126.121765	44.003098
3502.818122	731095.678244	44.008103
3502.218715	731064.777848	44.013108
3502.832335	731039.817919	44.018113
3502.364198	731017.363590	44.023117
3502.441354	730990.560626	44.028122
3502.665356	730962.643931	44.033127
3502.434992	730929.305238	44.038132
3502.346942	730894.209734	44.043137
3502.455149	730874.235119	44.048141
3502.636580	730848.454440	44.053146
3502.803948	730804.798856	44.058151
3502.487085	730772.563237	44.063156
3502.760615	730741.765380	44.068161
3502.401022	730726.274901	44.073165
3502.372449	730684.978478	44.078170
3502.669604	730661.159014	44.083175
3502.401605	730632.926076	44.088180
3502.672650	730597.076807	44.093185
3502.510880	730567.885212	44.098189
3502.754206	730533.872570	44.103194
3502.548074	730499.735751	44.108199
3502.536531	730484.880784	44.113204
3502.442636	730441.662482	44.118209
3502.485073	730425.015668	44.123213
3502.451959	730387.333695	44.128218
3502.508918	730366.970086	44.133223
3502.771457	730334.538208	44.138228
3502.782489	730294.619948	44.143233
3502.720424	730275.662403	44.148237
3502.632290	730242.000301	44.153242
3502.327982	730211.642318	44.158247
3502.299220	730181.734070	44.163252
3502.577377	730147.515972	44.168257
3502.546719	730138.111293	44.173261
3502.411772	730103.218197	44.178266
3502.517750	730068.334779	44.183271
3502.209713	730038.075813	44.188276
3502.449843	730007.924515	44.193281
3502.380240	730000.061403	44.198285
3502.120519	729972.022904	44.203290
3502.695896	729942.311388	44.208295
3502.351547	729920.378410	44.213300
3502.200132	729863.744787	44.218305
3502.178888	729852.159040	44.223309
3502.225918	729824.960976	44.228314
3502.384990	729813.791208	44.233319
3502.345905	729782.545956	44.238324
3502.767427	729756.078396	44.243329
3502.452796	729733.198990	44.248333
3502.527853	729703.370930	44.253338
3502.326959	729665.217975	44.258343
3502.454313	729650.190011	44.263348
3502.377799	729600.228523	44.268353
3502.245417	729587.571083	44.273357
3502.392720	729558.968805	44.278362
3502.522406	729534.529765	44.283367
3502.403004	729518.204934	44.288372
3502.383884	729471.403056	44.293377
3502.411137	729454.905346	44.298381
3502.546525	729430.316464	44.303386
3502.451637	729418.643175	44.308391
3502.253912	729380.587421	44.313396
3502.768427	729341.869300	44.318401
3502.142960	729322.705183	44.323405
3502.214763	729288.666067	44.328410
3501.968447	729257.948249	44.333415
3502.211751	729254.985920	44.338420
3502.106341	729219.093548	44.343425
3502.287357	729208.959485	44.348429
3502.332731	729172.843940	44.353434
3502.268364	729143.333989	44.358439
3502.270269	729128.672453	44.363444
3502.794326	729090.843135	44.368449
3502.741751	729065.343022	44.373453
3502.554012	729027.828822	44.378458
3502.653353	728999.083886	44.383463
3502.493645	728978.851568	44.388468
3502.748874	728935.617266	44.393473
3502.580466	728915.832018	44.398477
3502.306369	728885.414567	44.403482
3502.374741	728846.123678	44.408487
3502.229526	728826.136258	44.413492
3502.655017	728787.776910	44.418497
3502.375065	728776.678061	44.423501
3502.310896	728738.052427	44.428506
3502.725121	728714.802389	44.433511
3502.184901	728695.127402	44.438516
3502.301253	728661.177393	44.443521
3502.451907	728634.354553	44.448525
3502.388989	728616.037228	44.453530
3502.685434	728583.493724	44.458535
3502.523816	728552.115334	44.463540
3502.720790	728524.987293	44.468545
3502.413868	728501.855474	44.473549
3502.427950	728477.234172	44.478554
3502.500435	728434.324537	44.483559
3502.332333	728409.832120	44.488564
3502.500668	728382.014822	44.493569
3502.453382	728375.929756	44.498573
3502.202138	728322.967525	44.503578
3502.248795	728308.742968	44.508583
3502.314665	728287.282888	44.513588
3502.637453	728252.702728	44.518593
3502.506469	728226.172636	44.523597
3502.431292	728215.980482	44.528602
3502.428522	728170.852697	44.533607
3502.425445	728149.700840	44.538612
3502.599617	728116.630713	44.543617
3502.166760	728092.973569	44.548621
3502.400921	728080.352464	44.553626
3502.359927	728034.041314	44.558631
3502.233490	728029.356097	44.563636
3502.340680	727988.717155	44.568641
3502.345855	727963.550848	44.573645
3502.387591	727931.641179	44.578650
3502.751063	727909.536606	44.583655
3502.522446	727884.656273	44.588660
3502.685618	727847.029279	44.593665
3502.596417	727824.454133	44.598669
3502.541563	727779.877703	44.603674
3502.641012	727757.172208	44.608679
3502.492440	727725.293090	44.613684
3502.422464	727691.221131	44.618689
3502.746775	727663.474767	44.623693
3502.513528	727623.732289	44.628698
3502.262398	727600.638259	44.633703
3502.225334	727572.208020	44.638708
3502.518184	727552.293918	44.643713
3501.970376	727529.099946	44.648717
3502.274745	727503.486595	44.653722
3502.624483	727487.823514	44.658727
3502.274328	727459.345387	44.663732
3502.405455	727419.987754	44.668737
3502.641654	727401.667959	44.673741
3502.301571	727365.112508	44.678746
3502.488806	727340.657417	44.683751
3502.474463	727305.881092	44.688756
3502.629754	727274.643743	44.693761
3502.714245	727262.194668	44.698765
3502.300272	727223.966306	44.703770
3502.642355	727188.883041	44.708775
3502.317907	727166.840272	44.713780
3502.680561	727140.423489	44.718785
3502.364762	727110.501723	44.723789
3502.518089	727091.055384	44.728794
3502.265768	727051.808705	44.733799
3502.069336	727036.284299	44.738804
3502.755266	726999.706789	44.743809
3502.291526	726976.150581	44.748813
3502.214298	726948.170690	44.753818
3502.546646	726943.508343	44.758823
3502.270791	726914.124268	44.763828
3502.619648	726883.794887	44.768833
3502.319441	726845.595554	44.773837
3502.519364	726823.465457	44.778842
3502.518270	726786.901110	44.783847
3502.464622	726768.578113	44.788852
3502.413815	726723.747531	44.793857
3502.517249	726708.718100	44.798861
3502.710753	726679.008113	44.803866
3502.650590	726644.434713	44.808871
3502.411337	726619.998198	44.813876
3502.514543	726590.946877	44.818881
3502.219584	726569.938121	44.823885
3502.250309	726533.813324	44.828890
3502.188865	726507.712119	44.833895
3502.369008	726470.819214	44.838900
3502.450725	726443.306884	44.843905
3502.330565	726432.376700	44.848909
3502.326350	726402.500099	44.853914
3502.401344	726377.664245	44.858919
3502.115617	726354.423750	44.863924
3502.421488	726317.063503	44.868929
3502.025895	726295.723785	44.873933
3501.884346	726271.815166	44.878938
3502.482248	726250.410728	44.883943
3502.511637	726238.514215	44.888948
3502.473574	726200.169578	44.893953
3502.217457	726184.306545	44.898957
3502.496567	726151.904883	44.903962
3502.719623	726130.314150	44.908967
3502.154169	726104.146057	44.913972
3502.492427	726074.855979	44.918977
3502.335723	726048.769009	44.923981
3502.140800	726009.408775	44.928986
3502.398040	725987.613833	44.933991
3502.327060	725957.350207	44.938996
3502.531001	725934.027834	44.944001
3502.203691	725904.896368	44.949005
3502.216426	725886.560461	44.954010
3502.102368	725850.060099	44.959015
3501.968612	725851.568746	44.964020
3501.999595	725814.400160	44.969025
3502.255252	725806.429859	44.974029
3502.197377	725778.839199	44.979034
3502.222500	725749.896869	44.984039
3501.968638	725739.433757	44.989044
3502.312653	725701.420251	44.994049
3502.380239	725685.849780	44.999053
3502.235866	725648.263366	45.004058
3502.563431	725626.356773	45.009063
3502.336400	725614.749371	45.014068
3502.218073	725577.207892	45.019073
3502.190778	725548.669914	45.024077
3502.268972	725525.515761	45.029082
3502.323258	725489.283377	45.034087
3502.408019	725480.994045	45.039092
3502.313359	725444.488684	45.044097
3502.425273	725421.180021	45.049101
3502.141759	725394.913650	45.054106
3502.848506	725368.583138	45.059111
3502.448844	725337.082973	45.064116
3502.387978	725315.982874	45.069121
3502.783233	725299.267481	45.074125
3502.366096	725265.837292	45.079130
3502.710595	725239.169616	45.084135
3502.502308	725204.713666	45.089140
3502.885692	725173.331626	45.094145
3502.435213	725141.442640	45.099149
3502.448857	725122.708434	45.104154
3502.860106	725088.942808	45.109159
3502.740300	725060.170598	45.114164
3502.588434	725015.000440	45.119169
3502.428740	724984.301839	45.124173
3502.498135	724963.377597	45.129178
3502.519240	724931.707433	45.134183
3502.397736	724903.876535	45.139188
3502.795257	724875.563565	45.144193
3502.553769	724850.923916	45.149197
3502.184066	724819.416828	45.154202
3502.612090	724770.680752	45.159207
3502.219230	724767.078275	45.164212
3502.501586	724724.858002	45.169217
3502.622247	724706.253889	45.174221
3502.470242	724675.007726	45.179226
3502.416961	724641.762835	45.184231
3502.370358	724606.237005	45.189236
3502.463257	724581.045861	45.194241
3502.164983	724568.655773	45.199245
3502.387846	724545.722821	45.204250
3502.296489	724513.028834	45.209255
3501.923058	724494.356977	45.214260
3502.092596	724465.039414	45.219265
3502.061346	724453.596346	45.224269
3501.878657	724429.986501	45.229274
3501.859899	724408.431095	45.234279
3502.205724	724403.913782	45.239284
3502.511306	724366.990770	45.244289
3502.197210	724352.124949	45.249293
3502.236083	724323.571818	45.254298
3502.473196	724290.475902	45.259303
3502.387238	724260.704104	45.264308
3502.492036	724231.198133	45.269313
3502.630409	724218.735569	45.274317
3502.392918	724184.775769	45.279322
3502.432852	724148.738093	45.284327
3502.409607	724122.226523	45.289332
3502.480428	724089.999751	45.294337
3502.215932	724067.244897	45.299341
3502.202711	724036.320376	45.304346
3502.231101	724008.957376	45.309351
3502.661083	723989.904180	45.314356
3502.472693	723966.442632	45.319361
3502.499177	723933.479115	45.324365
3501.994689	723905.063628	45.329370
3502.320870	723872.843495	45.334375
3501.959978	723871.416132	45.339380
3502.291960	723833.346428	45.344385
3501.895857	723828.455418	45.349389
3501.960035	723787.356692	45.354394
3502.271689	723767.678154	45.359399
3502.041050	723745.214214	45.364404
3502.334176	723726.182961	45.369409
3502.020400	723702.344808	45.374413
3502.129630	723680.815976	45.379418
3502.237598	723655.322136	45.384423
3502.166019	723639.027259	45.389428
3502.257860	723615.766361	45.394433
3502.537348	723597.480531	45.399437
3502.586641	723567.832639	45.404442
3502.446743	723534.894945	45.409447
3502.282431	723519.358590	45.414452
3502.475634	723473.776164	45.419457
3502.232354	723459.690110	45.424461
3502.144805	723435.268686	45.429466
3502.243083	723403.232972	45.434471
3502.536118	723373.891185	45.439476
3502.643471	723349.982622	45.444481
3502.490725	723318.880137	45.449485
3502.392638	723297.037499	45.454490
3502.087007	723268.041813	45.459495
3502.351072	723247.328975	45.464500
3502.278212	723217.303417	45.469505
3502.290019	723202.332251	45.474509
3502.181001	723179.747595	45.479514
3502.246876	723150.442445	45.484519
3501.967861	723120.301800	45.489524
3502.333316	723091.591460	45.494529
3502.545776	723074.951260	45.499533
3502.121152	723056.135868	45.504538
3502.071851	723014.903293	45.509543
3501.919506	723002.784208	45.514548
3502.154322	722979.696235	45.519553
3502.102981	722940.248092	45.524557
3501.816817	722924.532419	45.529562
3502.167969	722920.756959	45.534567
3501.956174	722893.578545	45.539572
3502.021420	722871.757439	45.544577
3502.141715	722860.237621	45.549581
3502.364546	722827.881739	45.554586
3502.123686	722817.313621	45.559591
3502.210538	722794.100802	45.564596
3502.380777	722761.108919	45.569601
3502.283217	722742.387629	45.574605
3502.346544	722724.779900	45.579610
3502.368863	722692.902660	45.584615
3502.360385	722673.075988	45.589620
3502.427987	722638.216852	45.594625
3502.411720	722616.805069	45.599629
3502.475117	722595.826242	45.604634
3502.515680	722566.671908	45.609639
3502.366547	722546.421969	45.614644
3502.533668	722511.298045	45.619649
3502.333595	722474.846470	45.624653
3502.315801	722443.668882	45.629658
3502.461654	722410.729193	45.634663
3502.309462	722387.604194	45.639668
3502.255498	722372.047497	45.644673
3502.462041	722346.087229	45.649677
3502.250552	722310.281250	45.654682
3502.945322	722283.149743	45.659687
3502.366421	722258.756230	45.664692
3502.517968	722217.189147	45.669697
3502.804111	722195.676873	45.674701
3502.399066	722169.073225	45.679706
3502.530698	722134.498858	45.684711
3502.254281	722116.747521	45.689716
3502.387655	722078.553750	45.694721
3502.190372	722066.936436	45.699725
3502.403839	722025.259040	45.704730
3502.252737	722003.421719	45.709735
3502.236255	721987.560677	45.714740
3502.149366	721960.507337	45.719745
3502.369687	721949.911692	45.724749
3502.142543	721920.848769	45.729754
3502.372520	721893.990877	45.734759
3502.364068	721861.718907	45.739764
3502.188046	721843.355537	45.744769
3502.390597	721804.504626	45.749773
3502.285051	721790.045997	45.754778
3502.349603	721756.869228	45.759783
3502.116290	721744.662487	45.764788
3502.259745	721704.581446	45.769793
3502.249552	721689.313711	45.774797
3502.026829	721665.305942	45.779802
3502.417362	721643.328849	45.784807
3501.991671	721596.747381	45.789812
3502.398939	721512.845476	45.794817
3502.238668	721376.582711	45.799821
3501.941565	721189.372912	45.804826
3502.094314	720938.324132	45.809831
3501.699865	720639.362150	45.814836
3501.323222	720275.876997	45.819841
3501.365889	719862.174370	45.824845
3500.910044	719380.347283	45.829850
3500.643619	718854.769656	45.834855
3500.151345	718274.689640	45.839860
3499.495211	717631.405647	45.844865
3499.449840	716937.424707	45.849869
3499.012514	716174.196984	45.854874
3498.892204	715356.074157	45.859879
3497.966036	714486.599507	45.864884
3497.439800	713546.304329	45.869889
3496.851584	712567.699615	45.874893
3496.350231	711508.755512	45.879898
3495.502942	710407.838017	45.884903
3494.679210	709236.967279	45.889908
3494.242759	708001.368353	45.894913
3493.338023	706728.321155	45.899917
3492.152807	705393.489161	45.904922
3491.493154	703989.110511	45.909927
3490.325725	702542.501979	45.914932
3489.433414	701025.137438	45.919937
3488.281183	699461.872369	45.924941
3486.883356	697834.932689	45.929946
3486.406876	696168.158625	45.934951
3485.151039	694435.848132	45.939956
3484.049020	692645.172597	45.944961
3482.432902	690803.323445	45.949965
3481.226698	688918.578615	45.954970
3480.213005	686966.459407	45.959975
3478.746878	684975.857043	45.964980
3477.465299	682931.256054	45.969985
3475.608155	680824.878087	45.974989
3474.010598	678668.004431	45.979994
3472.809449	676462.872397	45.984999
3471.122501	674230.381341	45.990004
3470.026778	671926.014779	45.995009
3467.791084	669588.657360	46.000013
3466.120494	667200.399006	46.005018
3464.396218	664762.355144	46.010023
3462.397901	662277.123414	46.015028
3460.697120	659752.415013	46.020033
3458.699409	657187.802443	46.025037
3457.116794	654582.142846	46.030042
3455.093260	651921.411135	46.035047
3452.984164	649226.598607	46.040052
3451.083911	646509.181785	46.045057
3448.914162	643726.676375	46.050061
3446.399913	640914.757715	46.055066
3444.859217	638055.580620	46.060071
3442.482562	635174.782222	46.065076
3440.330579	632232.381650	46.070081
3437.801501	629269.541338	46.075085
3435.661534	626272.001299	46.080090
3433.467284	623223.380581	46.085095
3431.254238	620155.409524	46.090100
3428.757429	617045.065001	46.095105
3426.449288	613894.698371	46.100109
3423.884751	610719.905843	46.105114
3421.340962	607495.895925	46.110119
3418.855436	604269.903343	46.115124
3416.448247	600983.451024	46.120129
3414.029333	597663.375850	46.125133
3411.030861	594312.063157	46.130138
3408.532532	590931.277987	46.135143
3405.660828	587539.644064	46.140148
3402.907949	584113.002309	46.145153
3400.533535	580650.034178	46.150157
3397.597452	577158.520638	46.155162
3394.761551	573639.044419	46.160167
3391.587090	570104.348548	46.165172
3389.047913	566546.015896	46.170177
3386.077419	562955.151073	46.175181
3383.200814	559352.052280	46.180186
3380.613153	555695.880388	46.185191
3377.199650	552039.502902	46.190196
3373.968329	548350.958192	46.195201
3371.404455	544643.717540	46.200205
3368.083368	540907.069784	46.205210
3365.064841	537149.861134	46.210215
3361.799845	533391.002636	46.215220
3358.820611	529588.423472	46.220225
3355.419067	525779.683710	46.225229
3352.271809	521952.409783	46.230234
3349.076149	518102.207066	46.235239
3345.759628	514230.954753	46.240244
3342.379477	510353.349884	46.245249
3339.025074	506445.477478	46.250253
3335.986300	502531.048243	46.255258
3332.537586	498603.921392	46.260263
3329.094620	494654.018832	46.265268
3325.810562	490696.697510	46.270273
3322.355992	486718.965177	46.275277
3318.685389	482737.992543	46.280282
3315.090559	478739.973438	46.285287
3311.568906	474727.850877	46.290292
3308.330630	470700.584575	46.295297
3304.638331	466672.185550	46.300301
3301.136755	462628.881035	46.305306
3297.652284	458573.799237	46.310311
3293.930681	454513.633170	46.315316
3290.275936	450445.355089	46.320321
3286.912774	446369.802534	46.325325
3282.835761	442284.516596	46.330330
3279.782522	438189.476285	46.335335
3275.738244	434098.574472	46.340340
3272.170881	429986.263011	46.345345
3268.230311	425874.109718	46.350349
3264.408732	421755.984036	46.355354
3260.777867	417626.633178	46.360359
3257.152740	413525.383170	46.365364
3253.160761	409387.868212	46.370369
3249.808232	405253.243995	46.375373
3245.320386	401117.833622	46.380378
3241.998573	396972.305805	46.385383
3238.034978	392847.847596	46.390388
3234.249792	388706.659073	46.395393
3230.421227	384567.521304	46.400397
3226.363766	380428.500421	46.405402
3222.688320	376282.267260	46.410407
3218.604085	372136.137963	46.415412
3214.727907	367999.971992	46.420417
3210.843108	363857.014392	46.425421
3206.860059	359704.344708	46.430426
3203.116801	355579.291538	46.435431
3198.998800	351439.011533	46.440436
3195.456434	347299.212500	46.445441
3191.216696	343178.672038	46.450445
3187.197809	339051.253180	46.455450
3183.403999	334910.684673	46.460455
3179.088399	330785.711997	46.465460
3174.826042	326665.417808	46.470465
3171.170398	322561.667653	46.475469
3167.123991	318448.069142	46.480474
3163.076938	314341.986819	46.485479
3158.437479	310265.559373	46.490484
3154.788381	306178.776884	46.495489
3151.010174	302107.607019	46.500493
3147.045813	298030.281196	46.505498
3142.939551	293956.586255	46.510503
3138.724605	289899.189877	46.515508
3134.652149	285852.771708	46.520513
3130.780782	281806.133970	46.525517
3126.349795	277769.630606	46.530522
3122.511217	273732.086398	46.535527
3118.579706	269725.694462	46.540532
3114.194333	265708.712621	46.545537
3110.028346	261700.859709	46.550541
3105.795849	257713.124644	46.555546
3101.753563	253732.644692	46.560551
3097.478065	249762.306524	46.565556
3093.503886	245810.441471	46.570561
3089.470217	241852.267338	46.575565
3085.412261	237922.938176	46.580570
3081.374859	233986.068362	46.585575
3076.900542	230078.699600	46.590580
3072.814486	226170.226518	46.595585
3068.854146	222274.254075	46.600589
3064.316346	218398.805111	46.605594
3060.624702	214525.069421	46.610599
3056.397549	210651.251977	46.615604
3052.360898	206733.227003	46.620609
3047.937072	202902.821291	46.625613
3043.774464	199078.617750	46.630618
3039.842454	195269.085496	46.635623
3035.691175	191476.524302	46.640628
3031.382481	187684.962714	46.645633
3027.093280	183901.943715	46.650637
3023.032888	180148.783541	46.655642
3019.011092	176413.394611	46.660647
3014.549380	172678.065699	46.665652
3010.365370	168959.611139	46.670657
3006.517713	165263.397992	46.675661
3002.098462	161587.522369	46.680666
2998.386730	157913.554872	46.685671
2993.924001	154252.239502	46.690676
2989.701667	150611.750444	46.695681
2985.698947	146984.531834	46.700685
2981.114185	143375.923659	46.705690
2977.228266	139764.809128	46.710695
2972.688050	136180.264815	46.715700
2968.587000	132618.046359	46.720705
2964.561578	129067.657254	46.725709
2960.078925	125544.821746	46.730714
2955.935625	122013.975277	46.735719
2951.496421	118518.949627	46.740724
2947.342675	115037.418125	46.745729
2943.146955	111576.108190	46.750733
2938.698911	108135.641555	46.755738
2934.557781	104701.618453	46.760743
2929.889564	101291.177242	46.765748
2925.603401	97912.692734	46.770753
2921.344625	94543.076063	46.775757
2917.233282	91195.023047	46.780762
2913.023854	87860.111382	46.785767
2908.566921	84564.809322	46.790772
2903.512403	81286.885473	46.795777
2899.672059	78030.088525	46.800781
2894.981953	74793.052837	46.805786
2890.188169	71579.655822	46.810791
2885.450267	68394.502911	46.815796
2880.819743	65239.286177	46.820801
2875.996298	62123.903782	46.825805
2870.724711	59030.450287	46.830810
2866.435609	55980.898129	46.835815
2861.159812	52969.941023	46.840820
2855.586125	49990.735333	46.845825
2849.756611	47068.240570	46.850829
2842.411469	44246.960760	46.855834
2832.833664	41538.993127	46.860839
2822.761937	38932.262669	46.865844
2813.541206	36434.416874	46.870849
2804.292219	34042.804400	46.875853
2795.279869	31780.781064	46.880858
2787.309101	29621.616890	46.885863
2779.177284	27596.327526	46.890868
2771.676412	25672.959383	46.895873
2764.459673	23872.527274	46.900877
2757.264236	22175.211926	46.905882
2750.701692	20573.003141	46.910887
2744.444440	19061.290112	46.915892
2738.200481	17634.984853	46.920897
2732.474397	16285.716456	46.925901
2726.466672	15035.177816	46.930906
2721.216488	13833.273607	46.935911
2715.911224	12702.462090	46.940916
2710.900512	11623.960929	46.945921
2706.207448	10608.312238	46.950925
2701.319915	9641.968297	46.955930
2696.712289	8721.326885	46.960935
2692.282418	7853.690534	46.965940
2687.903949	7020.930539	46.970945
2683.281282	6234.234945	46.975949
2677.726827	5509.402063	46.980954
2672.522169	4818.094527	46.985959
2667.292399	4182.929312	46.990964
2662.044318	3603.653840	46.995969
2657.043279	3055.158025	47.000973
2651.788459	2560.772377	47.005978
2646.593323	2090.033642	47.010983
2641.782940	1674.866180	47.015988
2637.338577	1292.366817	47.020993
2632.700812	947.221371	47.025997
2627.915295	632.138151	47.031002
2623.412159	360.552867	47.036007
2617.538869	164.988246	47.041012
2604.139704	210.479123	47.046017
2596.391998	201.268731	47.051021
2591.971507	206.857442	47.056026
2590.247832	199.216962	47.061031
2589.721481	206.943748	47.066036
2589.148543	198.210921	47.071041
2587.752887	192.634369	47.076045
2585.211763	197.501077	47.081050
2582.125830	195.449931	47.086055
2578.664817	199.964644	47.091060
2575.775352	201.880583	47.096065
2572.655254	192.826920	47.101069
2569.299392	197.126352	47.106074
2565.994989	196.321759	47.111079
2562.917489	201.010787	47.116084
2559.495492	200.102663	47.121089
2556.762359	185.770227	47.126093
2553.527915	193.072886	47.131098
2550.271283	187.400514	47.136103
2546.700462	192.407972	47.141108
2543.601674	193.280403	47.146113
2540.546886	191.576200	47.151117
2537.358615	193.511677	47.156122
2534.004323	189.004942	47.161127
2530.069159	188.651994	47.166132
2526.572876	194.650444	47.171137
2523.849825	186.022273	47.176141
2520.257310	193.135006	47.181146
2517.117574	182.896443	47.186151
2513.220259	186.978408	47.191156
2510.112821	186.475048	47.196161
2507.060473	182.540715	47.201165
2503.900536	186.310155	47.206170
2500.425511	179.464960	47.211175
2496.772288	187.853072	47.216180
2492.921400	185.574409	47.221185
2489.374348	182.209170	47.226189
2486.242032	193.019116	47.231194
2482.920374	178.918264	47.236199
2479.688229	193.151377	47.241204
2475.846726	186.172897	47.246209
2472.301471	183.728953	47.251213
2468.720103	195.362132	47.256218
2465.760681	189.097090	47.261223
2462.402952	185.892634	47.266228
2458.659806	186.011463	47.271233
2455.847399	182.156556	47.276237
2452.142731	185.239998	47.281242
2449.103324	177.130610	47.286247
2445.585232	180.861716	47.291252
2441.520809	177.972644	47.296257
2438.060387	174.633404	47.301261
2434.842328	186.258133	47.306266
2431.534005	190.418967	47.311271
2427.939955	184.698183	47.316276
2424.227721	186.229036	47.321281
2421.211816	174.856124	47.326285
2417.750432	180.018470	47.331290
2414.112183	172.673192	47.336295
2410.712404	174.574590	47.341300
2406.465726	184.433021	47.346305
2403.533362	175.495718	47.351309
2400.220896	180.288543	47.356314
2396.781979	173.936939	47.361319
2393.468975	175.270287	47.366324
2390.173794	172.520296	47.371329
2386.753439	166.659975	47.376333
2382.455966	171.393596	47.381338
2379.036446	170.472167	47.386343
2376.470899	168.987464	47.391348
2372.798445	177.438225	47.396353
2369.257050	172.733587	47.401357
2365.464636	172.022320	47.406362
2361.907194	176.378045	47.411367
2358.764531	176.115629	47.416372
2355.065301	168.993989	47.421377
2351.900311	173.835710	47.426381
2348.130464	165.123138	47.431386
2344.477657	164.799111	47.436391
2341.403886	166.633910	47.441396
2337.294370	172.180365	47.446401
2334.319955	154.130399	47.451405
2331.000795	158.122377	47.456410
2327.370406	170.634576	47.461415
2323.924459	160.688464	47.466420
2319.935087	173.195007	47.471425
2316.686756	166.405089	47.476429
2313.290356	161.647158	47.481434
2309.704143	169.736401	47.486439
2306.659404	167.615290	47.491444
2302.386457	169.200318	47.496449
2299.387159	168.328962	47.501453
2295.683950	176.298013	47.506458
2292.435654	170.415671	47.511463
2289.158250	161.950227	47.516468
2285.620115	171.044888	47.521473
2282.179886	162.095614	47.526477
2278.313295	164.452270	47.531482
2275.125877	160.650116	47.536487
2271.602791	166.765037	47.541492
2268.016951	172.259821	47.546497
2264.318461	173.530600	47.551501
2260.842372	168.455909	47.556506
2257.475367	166.650695	47.561511
2254.046328	169.930709	47.566516
2250.273161	159.122039	47.571521
2247.280707	160.109511	47.576525
2243.964908	167.007607	47.581530
2240.144756	166.536444	47.586535
2236.725285	155.962047	47.591540
2233.340314	168.001411	47.596545
2229.683309	160.644191	47.601549
2226.083713	154.021470	47.606554
2222.380766	159.015034	47.611559
2218.919222	159.739168	47.616564
2215.594525	168.544458	47.621569
2212.271844	159.461575	47.626573
2208.843753	163.128247	47.631578
2205.135538	155.267607	47.636583
2201.924569	153.776292	47.641588
2198.150113	168.073411	47.646593
2194.550572	156.467093	47.651597
2191.108697	159.754002	47.656602
2187.839326	156.129628	47.661607
2184.345156	154.161544	47.666612
2180.802962	158.781278	47.671617
2177.471383	153.405140	47.676621
2173.676816	156.019745	47.681626
2170.607195	160.910551	47.686631
2166.950572	157.954189	47.691636
2162.927594	163.001626	47.696641
2159.588815	155.151856	47.701645
2156.258444	154.545028	47.706650
2152.510876	151.333143	47.711655
2149.636545	157.780493	47.716660
2145.342243	154.872805	47.721665
2142.460515	153.127459	47.726669
2138.719851	156.775931	47.731674
2135.315253	153.576693	47.736679
2131.748210	153.354898	47.741684
2128.253091	150.256456	47.746689
2125.230073	153.907997	47.751693
2121.195578	153.922059	47.756698
2117.868885	149.996392	47.761703
2114.345611	150.015044	47.766708
2110.658080	149.443742	47.771713
2107.132270	145.953536	47.776717
2103.763394	154.949705	47.781722
2100.499520	156.517269	47.786727
2097.098316	146.813400	47.791732
2093.202649	160.232897	47.796737
2089.926423	143.937200	47.801741
2086.423430	151.335174	47.806746
2082.781858	151.322075	47.811751
2079.131699	143.573917	47.816756
2075.713151	152.660398	47.821761
2072.722509	149.410412	47.826765
2069.003444	149.737308	47.831770
2065.179417	151.322014	47.836775
2062.393388	156.024952	47.841780
2058.332115	154.956150	47.846785
2054.645724	149.008002	47.851789
2051.332849	148.463875	47.856794
2047.619417	151.816644	47.861799
2044.628609	136.777283	47.866804
2040.951249	151.420764	47.871809
2037.490032	143.954024	47.876813
2033.843410	148.119658	47.881818
2030.191969	140.342154	47.886823
2027.116971	143.755661	47.891828
2023.327107	146.016366	47.896833
2019.883589	145.262950	47.901837
2016.218610	139.365965	47.906842
2012.709972	143.445875	47.911847
2009.339699	139.659902	47.916852
2005.814091	144.722999	47.921857
2003.060467	139.978346	47.926861
1998.878091	148.479217	47.931866
1995.503364	144.188801	47.936871
1991.874093	150.968313	47.941876
1988.180096	142.636640	47.946881
1985.062365	150.212200	47.951885
1981.198704	144.834495	47.956890
1978.031352	148.500092	47.961895
1974.528064	143.127801	47.966900
1970.828152	140.306820	47.971905
1967.664982	142.510439	47.976909
1963.684817	147.758161	47.981914
1960.344768	139.538162	47.986919
1956.923834	140.492580	47.991924
1953.363178	149.527024	47.996929
1950.140304	145.028826	48.001933
1946.708042	138.919410	48.006938
1943.198129	142.102871	48.011943
1939.450514	138.808682	48.016948
1935.560649	145.970695	48.021953
1932.311167	146.216784	48.026957
1928.889842	139.040736	48.031962
1925.328228	137.221137	48.036967
1921.916685	143.566109	48.041972
1918.180279	144.275863	48.046977
1914.833607	132.544764	48.051981
1911.528000	151.545135	48.056986
1908.093633	145.253754	48.061991
1904.766809	132.536836	48.066996
1900.890873	149.479239	48.072001
1897.660537	135.843759	48.077005
1893.866812	149.463221	48.082010
1890.551544	138.239636	48.087015
1886.943496	141.303380	48.092020
1882.896642	140.583216	48.097025
1880.164222	139.143716	48.102029
1876.445591	142.880305	48.107034
1872.760466	141.702369	48.112039
1869.497389	137.400712	48.117044
1865.415555	152.295031	48.122049
1862.224831	140.504071	48.127053
1858.875345	137.270285	48.132058
1855.144662	142.242640	48.137063
1852.287202	133.547351	48.142068
1848.048407	141.673438	48.147073
1845.264538	133.367187	48.152077
1841.673060	148.058763	48.157082
1838.055870	143.762340	48.162087
1834.612613	135.207438	48.167092
1830.585579	139.418887	48.172097
1827.537238	132.537310	48.177101
1824.090282	134.173977	48.182106
1820.387115	145.368234	48.187111
1817.035451	139.827557	48.192116
1812.971415	144.763445	48.197121
1809.987272	138.677203	48.202125
1806.437194	123.908230	48.207130
1802.936994	137.122071	48.212135
1799.479027	137.726522	48.217140
1795.617610	148.717237	48.222145
1792.242188	137.226607	48.227149
1788.812719	136.559447	48.232154
1785.436198	147.181557	48.237159
1782.333153	136.753404	48.242164
1778.310713	144.378287	48.247169
1774.890441	137.677971	48.252173
1771.549634	143.296202	48.257178
1767.861824	140.371361	48.262183
1764.557534	139.432130	48.267188
1760.653482	142.806733	48.272193
1757.195592	134.660633	48.277197
1753.585707	135.803294	48.282202
1750.048466	141.688032	48.287207
1747.050127	143.165392	48.292212
1743.543408	139.621994	48.297217
1740.344080	135.628011	48.302221
1736.576921	136.492371	48.307226
1732.568517	137.403300	48.312231
1729.502998	132.290019	48.317236
1725.713168	141.885809	48.322241
1722.405800	138.334950	48.327245
1718.402236	139.300148	48.332250
1715.140243	139.057475	48.337255
1712.006501	124.313935	48.342260
1708.570472	137.964399	48.347265
1704.774086	129.192465	48.352269
1701.329354	137.178599	48.357274
1697.962694	139.879162	48.362279
1694.366898	124.131154	48.367284
1690.691566	127.065847	48.372289
1687.421443	133.619081	48.377293
1684.039073	137.002276	48.382298
1680.472921	134.161602	48.387303
1676.833531	125.910383	48.392308
1673.140601	137.271764	48.397313
1670.136044	127.682498	48.402317
1666.093806	137.266748	48.407322
1662.720805	135.076768	48.412327
1659.163146	122.722430	48.417332
1655.535583	127.318736	48.422337
1652.151738	125.323159	48.427341
1648.831771	132.117905	48.432346
1645.344011	132.769424	48.437351
1642.217745	125.396463	48.442356
1638.347587	137.381137	48.447361
1635.420146	122.051228	48.452365
1631.711364	122.616531	48.457370
1627.587266	134.115092	48.462375
1624.408944	129.680423	48.467380
1620.467731	136.653812	48.472385
1617.090973	129.304497	48.477389
1613.623045	129.772987	48.482394
1610.272014	122.577695	48.487399
1607.055477	113.415226	48.492404
1603.041294	125.785828	48.497409
1599.396082	126.730396	48.502413
1596.393684	123.619825	48.507418
1592.584711	125.838828	48.512423
1589.419983	122.573929	48.517428
1585.617996	132.688056	48.522433
1582.624916	119.856085	48.527437
1578.700946	126.865134	48.532442
1575.434218	128.014572	48.537447
1572.013274	122.545135	48.542452
1567.880912	125.359682	48.547457
1564.740193	113.050996	48.552461
1561.385244	124.526107	48.557466
1557.604527	120.348111	48.562471
1554.209447	121.818924	48.567476
1550.748677	117.696206	48.572481
1547.153674	122.093818	48.577485
1543.621772	120.251255	48.582490
1540.183010	122.539366	48.587495
1536.882784	119.968041	48.592500
1533.174804	129.984774	48.597505
1529.889014	125.559646	48.602509
1526.505931	119.511908	48.607514
1523.189968	113.037886	48.612519
1519.318307	112.723823	48.617524
1515.590035	124.617440	48.622529
1512.109865	113.295536	48.627533
1508.666303	120.017254	48.632538
1505.465124	121.665235	48.637543
1501.619366	120.066581	48.642548
1497.840872	124.324447	48.647553
1494.785964	118.159354	48.652557
1491.221376	116.024847	48.657562
1487.772791	120.444482	48.662567
1484.194087	121.093783	48.667572
1480.142634	128.951018	48.672577
1477.027203	125.150766	48.677581
1473.898355	121.903306	48.682586
1470.041677	122.078178	48.687591
1466.966264	114.905338	48.692596
1463.213022	130.012616	48.697601
1459.561956	122.338164	48.702605
1456.319253	120.070369	48.707610
1452.637419	118.666078	48.712615
1449.153713	117.724757	48.717620
1445.453518	125.231710	48.722625
1442.332106	119.722149	48.727629
1438.758646	120.678268	48.732634
1435.096732	122.175899	48.737639
1431.958396	126.632706	48.742644
1428.146570	119.931282	48.747649
1424.511237	111.966351	48.752653
1420.886611	122.120739	48.757658
1417.632348	123.240796	48.762663
1413.968530	122.031290	48.767668
1410.457313	124.402314	48.772673
1407.202055	120.711459	48.777677
1403.374746	125.136125	48.782682
1399.896875	124.728464	48.787687
1396.549245	110.855485	48.792692
1393.129823	118.480054	48.797697
1389.841315	119.259068	48.802701
1386.457223	112.518958	48.807706
1382.875760	121.725334	48.812711
1379.212208	119.575106	48.817716
1375.370641	120.656890	48.822721
1372.337310	109.786962	48.827725
1368.665215	118.731857	48.832730
1365.231013	120.648149	48.837735
1361.653893	122.784613	48.842740
1358.248844	120.102477	48.847745
1354.746370	116.911727	48.852749
1350.833147	131.710641	48.857754
1347.252032	124.715997	48.862759
1344.101553	118.733954	48.867764
1340.452710	114.897845	48.872769
1336.892322	119.318107	48.877773
1333.759009	112.639598	48.882778
1330.100385	121.204394	48.887783
1326.720293	119.851169	48.892788
1323.085920	125.053681	48.897793
1319.758718	121.522786	48.902797
1315.829983	117.592852	48.907802
1312.149211	120.827500	48.912807
1309.104302	116.080336	48.917812
1305.626295	117.516686	48.922817
1302.037692	109.071320	48.927821
1298.579042	116.397550	48.932826
1295.184791	110.757768	48.937831
1291.389176	121.155013	48.942836
1288.074201	119.064656	48.947841
1284.562930	121.862818	48.952845
1280.980346	125.217817	48.957850
1277.341967	116.889034	48.962855
1274.174364	119.080613	48.967860
1270.534871	116.994777	48.972865
1266.974617	116.876516	48.977869
1263.509531	124.758550	48.982874
1259.902434	126.061168	48.987879
1256.691346	108.506523	48.992884
1253.066281	113.503498	48.997889
1249.673019	119.664335	49.002893
1245.792525	111.835205	49.007898
1242.187937	118.002761	49.012903
1239.247223	119.957546	49.017908
1235.074962	118.789613	49.022913
1232.067081	106.512130	49.027917
1228.749476	113.853767	49.032922
1225.255664	120.683244	49.037927
1221.903549	116.304641	49.042932
1218.058828	120.352259	49.047937
1214.201095	110.292055	49.052941
1210.803680	106.404625	49.057946
1206.928223	117.725837	49.062951
1204.060044	107.108958	49.067956
1200.471443	129.263117	49.072961
1197.024161	109.545686	49.077965
1193.348543	118.003076	49.082970
1189.728111	119.855364	49.087975
1186.565172	116.930473	49.092980
1182.626388	120.111773	49.097985
1179.576617	115.941926	49.102989
1176.452765	114.871861	49.107994
1172.701529	115.004292	49.112999
1169.054300	115.146763	49.118004
1165.459408	113.634599	49.123009
1161.640931	111.366307	49.128013
1158.487086	110.616754	49.133018
1154.913580	112.409807	49.138023
1151.291353	107.630530	49.143028
1147.814367	116.111550	49.148033
1144.468859	111.809075	49.153037
1140.873176	111.120153	49.158042
1137.409732	113.865128	49.163047
1134.180742	111.910845	49.168052
1130.262961	113.408986	49.173057
1127.050259	111.174362	49.178061
1123.719744	111.604318	49.183066
1119.521052	118.556726	49.188071
1115.964303	114.718011	49.193076
1112.895993	119.063195	49.198081
1109.351045	110.730563	49.203085
1106.019461	106.205788	49.208090
1102.754571	114.808256	49.213095
1098.994201	117.547496	49.218100
1095.108868	121.221858	49.223105
1091.651470	110.528039	49.228109
1088.617895	109.104874	49.233114
1084.870340	120.453573	49.238119
1081.294341	115.080424	49.243124
1077.364441	115.804884	49.248129
1074.057678	108.586530	49.253133
1071.122733	108.896259	49.258138
1067.205570	108.509591	49.263143
1064.048128	118.481989	49.268148
1060.458179	126.360931	49.273153
1056.666418	122.236898	49.278157
1053.247129	121.328449	49.283162
1049.602154	120.402263	49.288167
1046.293675	110.539906	49.293172
1042.724622	118.003362	49.298177
1038.785727	119.668467	49.303181
1036.361150	120.225549	49.308186
1032.450827	118.594955	49.313191
1029.104034	118.007838	49.318196
1025.543055	125.896617	49.323201
1021.707684	121.719639	49.328205
1018.077477	120.775053	49.333210
1014.360916	123.498632	49.338215
1011.523318	113.852664	49.343220
1007.733378	119.646700	49.348225
1004.643601	110.175840	49.353229
1000.943663	110.558244	49.358234
997.217792	117.567941	49.363239
993.692964	102.344853	49.368244
990.017743	116.723790	49.373249
986.751397	119.354192	49.378253
983.581682	114.176990	49.383258
979.700511	116.260227	49.388263
976.549236	118.362874	49.393268
972.341887	118.240558	49.398273
969.365747	114.994258	49.403277
965.976641	111.881376	49.408282
962.119355	113.706509	49.413287
959.094371	101.666117	49.418292
955.114776	123.556698	49.423297
951.092178	113.380152	49.428301
948.269081	111.741910	49.433306
944.630495	112.124081	49.438311
941.573860	110.741536	49.443316
937.908505	117.512359	49.448321
934.456158	108.967626	49.453325
931.040652	112.494565	49.458330
927.057288	116.472401	49.463335
923.651614	107.568899	49.468340
919.975655	114.265908	49.473345
916.131844	107.960183	49.478349
913.230838	117.838755	49.483354
910.001332	111.775986	49.488359
906.104256	106.678883	49.493364
902.262266	109.797640	49.498369
899.070452	103.144141	49.503373
895.445555	104.561088	49.508378
891.902190	109.914234	49.513383
888.691722	104.507636	49.518388
884.993787	111.076485	49.523393
881.754530	104.515699	49.528397
878.244316	107.431206	49.533402
874.960089	111.703321	49.538407
871.700207	106.000025	49.543412
867.763299	103.125827	49.548417
864.248962	107.894419	49.553421
860.743155	113.975664	49.558426
856.889886	110.312702	49.563431
853.302761	97.722849	49.568436
850.097738	104.723861	49.573441
846.559064	109.810848	49.578445
843.371841	99.500986	49.583450
839.551869	110.671009	49.588455
836.309880	110.320872	49.593460
832.832091	118.141559	49.598465
829.105603	115.006641	49.603469
825.626378	109.485688	49.608474
821.767424	111.752459	49.613479
818.294719	94.807852	49.618484
815.057401	105.634845	49.623489
811.801823	102.802517	49.628493
808.121144	99.480467	49.633498
804.356828	105.978658	49.638503
801.106040	103.572580	49.643508
797.735009	100.938541	49.648513
794.212891	103.565602	49.653517
790.928718	105.481576	49.658522
786.801029	111.280936	49.663527
783.728905	104.459332	49.668532
780.021821	112.989516	49.673537
776.660902	106.882880	49.678541
772.898222	103.096477	49.683546
769.266526	103.832460	49.688551
766.216551	102.275084	49.693556
762.588280	111.192243	49.698561
758.555957	103.497822	49.703565
755.446710	94.459004	49.708570
751.957014	110.873115	49.713575
748.789661	100.348304	49.718580
745.282264	104.466798	49.723585
741.601630	101.913618	49.728589
738.493179	98.704370	49.733594
734.412722	102.365327	49.738599
730.803797	97.408982	49.743604
727.415821	100.839556	49.748609
723.823646	108.106175	49.753613
720.677370	94.338838	49.758618
717.182832	106.943219	49.763623
713.888629	96.884416	49.768628
709.959313	96.382068	49.773633
706.129428	104.509728	49.778637
703.122342	94.346013	49.783642
699.004851	94.568045	49.788647
696.104522	94.971356	49.793652
692.481594	102.966515	49.798657
688.721434	106.611230	49.803661
685.790346	99.977521	49.808666
681.968776	96.790582	49.813671
678.797528	104.841270	49.818676
674.492697	100.575532	49.823681
671.422848	107.417150	49.828685
668.301081	103.662549	49.833690
664.186028	106.248092	49.838695
661.210372	107.140650	49.843700
657.655740	102.410609	49.848705
653.724176	103.222542	49.853709
650.565270	101.851203	49.858714
646.800303	108.695555	49.863719
643.527110	102.018821	49.868724
639.843252	105.837631	49.873729
636.091852	108.032695	49.878733
633.274967	108.675028	49.883738
629.437501	109.990802	49.888743
625.705898	102.413707	49.893748
622.325951	102.703621	49.898753
618.958298	100.821407	49.903757
615.706342	101.566913	49.908762
611.821878	109.096281	49.913767
608.432592	98.770122	49.918772
604.505157	110.083999	49.923777
601.282617	108.516810	49.928781
598.237764	97.877137	49.933786
594.193522	108.713457	49.938791
590.792269	101.811088	49.943796
587.278544	102.693265	49.948801
584.067830	100.526801	49.953805
580.474674	108.461471	49.958810
577.239828	103.450468	49.963815
573.652974	100.927107	49.968820
569.758343	106.207779	49.973825
566.342046	105.994034	49.978829
562.810370	100.199797	49.983834
558.955872	100.663594	49.988839
555.805567	99.930465	49.993844
552.009997	109.443389	49.998849
549.032307	105.427052	50.003853
545.574520	102.016056	50.008858
541.942967	104.099804	50.013863
538.656841	101.421927	50.018868
534.802831	96.350808	50.023873
531.287489	104.286450	50.028877
527.746802	101.048042	50.033882
524.058715	92.075002	50.038887
521.072038	88.939896	50.043892
517.388329	97.587566	50.048897
513.753954	100.194939	50.053901
510.499105	105.103588	50.058906
506.472997	102.615475	50.063911
503.192635	96.552179	50.068916
499.677890	101.028658	50.073921
496.190146	100.756145	50.078925
492.748267	96.152830	50.083930
489.191891	103.459479	50.088935
486.215007	95.212193	50.093940
482.532215	103.753574	50.098945
478.738086	103.417717	50.103949
475.200486	97.934157	50.108954
471.597928	97.734536	50.113959
468.214782	93.000754	50.118964
464.667238	102.429481	50.123969
461.169927	86.321662	50.128973
457.621575	86.619642	50.133978
454.371603	87.500902	50.138983
450.758519	89.490695	50.143988
447.219943	90.519375	50.148993
443.631450	95.043818	50.153997
440.756618	96.114411	50.159002
436.705132	104.265735	50.164007
433.402452	97.024744	50.169012
429.634551	97.828540	50.174017
426.398236	99.317720	50.179021
422.707854	95.340885	50.184026
418.822822	96.666292	50.189031
415.618362	92.641014	50.194036
412.088462	88.663482	50.199041
408.919060	97.053844	50.204045
405.465861	86.935984	50.209050
401.464830	96.928602	50.214055
398.199201	91.425755	50.219060
394.908980	91.410124	50.224065
391.197312	96.846158	50.229069
387.658725	89.011992	50.234074
384.018423	98.327661	50.239079
380.841846	90.830230	50.244084
377.258171	90.306500	50.249089
373.201698	94.820834	50.254093
370.229961	93.181529	50.259098
366.849439	93.894625	50.264103
363.528602	88.815545	50.269108
359.992514	101.435719	50.274113
355.867404	100.888941	50.279117
352.650953	92.952943	50.284122
349.136072	106.121564	50.289127
346.087416	96.137485	50.294132
342.418713	103.869147	50.299137
338.358925	93.839705	50.304141
335.120336	89.205640	50.309146
331.204580	98.775523	50.314151
328.253281	92.562989	50.319156
324.787290	93.238365	50.324161
321.003943	85.510486	50.329165
317.968810	97.416102	50.334170
313.948305	101.414625	50.339175
310.702759	92.015309	50.344180
306.876959	87.617189	50.349185
303.373940	93.511500	50.354189
300.157637	89.563656	50.359194
296.403288	102.904754	50.364199
293.100879	106.222031	50.369204
289.492204	97.535619	50.374209
286.025963	97.856260	50.379213
282.924961	91.106532	50.384218
278.858268	99.277674	50.389223
275.607327	92.177439	50.394228
272.150969	89.791197	50.399233
268.080949	93.148330	50.404237
265.299457	84.777514	50.409242
261.282111	95.942351	50.414247
258.191083	97.964681	50.419252
254.283195	104.829252	50.424257
251.058594	99.651253	50.429261
248.004496	93.200248	50.434266
243.859895	91.543246	50.439271
240.701462	92.009318	50.444276
237.295691	90.204564	50.449281
233.557779	103.441952	50.454285
230.549647	94.535810	50.459290
226.509433	94.385757	50.464295
222.810389	97.245806	50.469300
219.635902	98.146911	50.474305
216.111794	90.541582	50.479309
212.668535	88.207489	50.484314
208.647625	101.041819	50.489319
205.257025	92.255058	50.494324
201.994128	98.994544	50.499329
198.638227	99.418942	50.504333
195.458792	88.823197	50.509338
191.245723	106.941805	50.514343
187.954421	98.421989	50.519348
184.402818	101.477691	50.524353
180.866563	95.785783	50.529357
177.788479	95.431897	50.534362
173.640816	96.197355	50.539367
170.128499	95.677180	50.544372
166.977619	94.921346	50.549377
163.440729	94.258823	50.554381
160.162836	95.822572	50.559386
156.332775	99.465486	50.564391
153.179582	101.161726	50.569396
150.002261	89.609586	50.574401
145.772551	99.617188	50.579405
142.460966	90.219282	50.584410
138.597989	99.566082	50.589415
135.251140	90.723597	50.594420
131.747769	86.482224	50.599425
128.324554	98.412341	50.604429
125.403062	81.287581	50.609434
121.277986	89.096150	50.614439
117.929993	92.896282	50.619444
114.576050	94.460224	50.624449
110.978449	99.338877	50.629453
107.812618	93.795866	50.634458
103.946196	100.598444	50.639463
100.493035	96.396735	50.644468
96.953499	93.522392	50.649473
93.288929	97.321876	50.654477
89.757987	95.719711	50.659482
86.154479	101.231028	50.664487
82.709859	95.027742	50.669492
79.293264	97.940010	50.674497
75.952424	100.626617	50.679501
72.483795	96.267653	50.684506
69.132985	104.032535	50.689511
65.760030	101.654755	50.694516
61.904527	92.082157	50.699521
58.327861	103.850661	50.704525
55.169821	88.151592	50.709530
51.457623	93.877871	50.714535
47.788111	87.474069	50.719540
44.249530	87.693812	50.724545
40.432708	100.481263	50.729549
37.227713	86.117059	50.734554
33.516261	98.978630	50.739559
30.137724	99.740205	50.744564
26.818641	87.546238	50.749569
23.325394	96.763629	50.754573
20.020652	87.970910	50.759578
16.270021	95.569177	50.764583
12.882418	82.785690	50.769588
9.500345	94.322298	50.774593
5.725033	91.735324	50.779597
2.459575	89.131808	50.784602