Tue Jun 21 11:08:00 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.517662	84.177452	0.000000
0.574647	94.437907	0.005005
0.718061	81.727616	0.010010
0.498812	84.356346	0.015014
0.385910	68.017118	0.020019
0.173208	62.646044	0.025024
-0.148273	66.190752	0.030029
-0.135652	47.192016	0.035034
-0.503289	44.321166	0.040038
-0.996297	38.768994	0.045043
-0.940254	21.066486	0.050048
-1.390129	24.280602	0.055053
-1.577276	11.818693	0.060058
-1.906464	-0.427481	0.065062
-2.139235	10.556175	0.070067
-2.247072	0.602661	0.075072
-2.800485	-6.699500	0.080077
-3.390280	-11.905882	0.085082
-3.545623	-3.229641	0.090086
-3.694628	-14.698946	0.095091
-4.452673	-7.123863	0.100096
-5.209495	-7.147074	0.105101
-5.134093	-0.833029	0.110106
-4.438801	-10.519148	0.115110
-5.326516	-9.962034	0.120115
-5.051103	-15.353333	0.125120
-5.200493	-11.221661	0.130125
-5.574998	-12.616302	0.135130
-6.368999	-17.953242	0.140134
-6.836629	-4.109836	0.145139
-6.520734	-13.338853	0.150144
-6.915859	-5.208192	0.155149
-7.039057	-0.507604	0.160154
-6.799032	-10.425380	0.165158
-7.758057	-13.292213	0.170163
-8.037006	-15.067151	0.175168
-8.416353	-10.074126	0.180173
-8.416115	-12.865780	0.185178
-8.590965	-7.849591	0.190182
-8.762917	-9.140037	0.195187
-8.509975	-8.603890	0.200192
-9.624686	-10.362374	0.205197
-9.954159	-12.567616	0.210202
-9.938211	-9.135438	0.215206
-10.335374	-8.127553	0.220211
-10.255384	-8.131279	0.225216
-10.093719	-4.744544	0.230221
-10.575535	-8.681607	0.235226
-11.277349	-10.870573	0.240230
-11.771515	-10.146569	0.245235
-11.670770	-12.208358	0.250240
-11.831615	-10.518160	0.255245
-12.202871	-5.311776	0.260250
-11.512717	-6.618501	0.265254
-12.564818	-15.044168	0.270259
-13.070430	-15.819968	0.275264
-13.561706	-14.036175	0.280269
-13.510582	-13.109631	0.285274
-13.359739	-14.733548	0.290278
-13.609490	-10.581704	0.295283
-13.585403	-15.648604	0.300288
-14.219911	-13.105435	0.305293
-14.902031	-16.041211	0.310298
-14.755408	-20.216134	0.315302
-15.061390	-17.111891	0.320307
-15.400327	-11.669721	0.325312
-15.831344	-9.500254	0.330317
-16.227997	-4.132982	0.335322
-16.159096	-9.378984	0.340326
-16.392793	-3.672646	0.345331
-16.188739	-6.064514	0.350336
-16.511993	-16.075877	0.355341
-17.401766	-7.832912	0.360346
-17.476473	-10.470470	0.365350
-17.958383	2.057520	0.370355
-17.962042	-7.287893	0.375360
-17.991258	-8.896594	0.380365
-18.315034	-7.890008	0.385370
-18.445662	-5.016082	0.390374
-19.137359	4.348286	0.395379
-19.608295	-5.813858	0.400384
-19.713046	-6.369910	0.405389
-19.775387	-13.688467	0.410394
-19.468079	-16.331075	0.415398
-19.853749	-4.274274	0.420403
-19.946527	-13.388450	0.425408
-20.461036	-7.676457	0.430413
-20.985791	-17.103299	0.435418
-20.835462	-9.653192	0.440422
-21.333818	-8.608814	0.445427
-21.498207	-9.838944	0.450432
-22.497127	-7.073020	0.455437
-22.662149	-8.621146	0.460442
-22.877000	-16.760408	0.465446
-22.754880	-10.653609	0.470451
-22.553989	-9.860795	0.475456
-23.084529	-5.401575	0.480461
-23.376025	-8.252463	0.485466
-23.114496	-16.606777	0.490470
-23.651624	-8.232773	0.495475
-24.219588	-13.184062	0.500480
-24.434453	-8.524141	0.505485
-24.397246	-6.001635	0.510490
-24.240313	-10.478608	0.515494
-25.354622	1.686236	0.520499
-25.814369	-12.944970	0.525504
-26.027676	-4.573088	0.530509
-26.165862	-3.973746	0.535514
-25.932595	-10.080896	0.540518
-26.241234	-11.862953	0.545523
-26.011862	-10.789119	0.550528
-26.895836	-9.022183	0.555533
-27.501445	-10.899507	0.560538
-27.526463	-17.268759	0.565542
-27.750959	-11.104359	0.570547
-27.645868	-20.085737	0.575552
-27.863641	-10.053947	0.580557
-28.581055	-7.342929	0.585562
-28.726841	-17.903058	0.590566
-28.931969	-3.073642	0.595571
-29.111874	-8.571676	0.600576
-29.081315	-13.227025	0.605581
-29.348797	-8.367570	0.610586
-30.259609	-11.583767	0.615590
-30.614402	-7.943772	0.620595
-30.747568	-10.474758	0.625600
-30.874390	-7.284349	0.630605
-30.976131	-3.128598	0.635610
-30.947297	-7.405575	0.640614
-31.095968	-2.733132	0.645619
-30.998018	-6.326944	0.650624
-31.493796	-9.781186	0.655629
-32.166503	-4.832716	0.660634
-32.517861	-7.031372	0.665638
-32.755654	-8.179095	0.670643
-33.597262	-8.583911	0.675648
-33.616392	-14.609793	0.680653
-33.560593	-10.875984	0.685658
-33.835652	-9.216993	0.690662
-34.341392	-6.507088	0.695667
-34.291760	-12.911988	0.700672
-34.621833	1.514452	0.705677
-34.531273	-8.132300	0.710682
-34.358396	-15.063176	0.715686
-34.795550	-1.603694	0.720691
-35.122244	-4.112497	0.725696
-35.376710	3.397548	0.730701
-35.927997	-6.001223	0.735706
-36.021245	-1.613829	0.740710
-37.082415	1.697377	0.745715
-37.128233	-7.328871	0.750720
-36.702615	-2.110402	0.755725
-37.143728	-4.683925	0.760730
-37.421367	-10.606021	0.765734
-37.827560	-6.037943	0.770739
-37.701017	-10.161394	0.775744
-37.400265	-11.225837	0.780749
-38.371150	-9.273221	0.785754
-38.659693	-8.572611	0.790758
-38.888781	-5.968116	0.795763
-39.085421	-12.286056	0.800768
-40.018149	-9.683431	0.805773
-40.004760	-10.682523	0.810778
-39.664723	-11.868714	0.815782
-40.574952	-2.789810	0.820787
-40.316071	-14.837554	0.825792
-40.417950	-13.976840	0.830797
-40.955946	-8.994835	0.835802
-40.716969	-7.813073	0.840806
-41.562987	-7.226154	0.845811
-41.690124	-8.338133	0.850816
-42.000346	1.584655	0.855821
-42.330600	-5.091025	0.860826
-41.930573	-9.026324	0.865830
-42.533698	-0.852728	0.870835
-42.725396	-18.803444	0.875840
-43.288770	-4.423423	0.880845
-43.261355	-2.719805	0.885850
-43.377064	-1.981711	0.890854
-44.092634	-4.519646	0.895859
-44.811696	-15.494346	0.900864
-44.812299	-9.665195	0.905869
-44.978766	-5.157341	0.910874
-45.211090	-5.623988	0.915878
-45.424850	-6.748064	0.920883
-45.420585	-3.185686	0.925888
-45.354143	1.024698	0.930893
-45.449157	-9.789522	0.935898
-45.892217	-16.084212	0.940902
-46.761961	-7.932570	0.945907
-46.760602	-9.229616	0.950912
-46.974487	-10.800826	0.955917
-46.960550	-17.422404	0.960922
-47.077161	-11.162603	0.965926
-48.478903	0.788380	0.970931
-47.986299	-8.341639	0.975936
-48.316091	-0.688684	0.980941
-48.657317	-5.091839	0.985946
-48.293695	-14.252984	0.990950
-48.487263	-3.490333	0.995955
-48.902494	-3.392509	1.000960
-49.901423	-8.352934	1.005965
-50.329462	-8.006126	1.010970
-49.974698	-9.500227	1.015974
-49.989127	-10.508920	1.020979
-50.226894	-11.658225	1.025984
-50.113838	-4.623054	1.030989
-50.879768	-2.032658	1.035994
-51.174919	-15.879485	1.040998
-51.456860	-9.498570	1.046003
-51.732348	-10.339906	1.051008
-51.723672	-10.267690	1.056013
-52.363997	-14.021811	1.061018
-52.607199	-13.318843	1.066022
-52.881316	-16.874121	1.071027
-52.904464	-14.252427	1.076032
-52.802702	-13.422084	1.081037
-53.415745	-15.391510	1.086042
-53.807029	-12.277480	1.091046
-54.269854	-12.225053	1.096051
-54.342863	-16.770501	1.101056
-54.396496	-9.795934	1.106061
-54.907569	-8.812987	1.111066
-54.360386	-14.120240	1.116070
-55.153672	-7.097964	1.121075
-55.865113	-18.689400	1.126080
-55.839123	-18.663266	1.131085
-56.088354	-11.373134	1.136090
-56.247986	-6.346442	1.141094
-56.314875	-7.070773	1.146099
-56.328541	-6.680111	1.151104
-57.112628	-9.750149	1.156109
-57.837008	9.773183	1.161114
-57.473118	-18.346532	1.166118
-57.752715	0.146064	1.171123
-57.852725	-9.793341	1.176128
-57.966276	-9.754950	1.181133
-58.224343	-2.803552	1.186138
-58.646516	-6.203677	1.191142
-59.314149	-0.158875	1.196147
-59.511544	-8.168618	1.201152
-59.228276	-6.752066	1.206157
-59.968409	-14.123730	1.211162
-59.618425	-2.018665	1.216166
-60.462230	-7.195795	1.221171
-60.958553	-7.456512	1.226176
-61.027327	-4.043851	1.231181
-61.231728	-4.947871	1.236186
-60.989515	-10.629869	1.241190
-61.282030	-11.515152	1.246195
-61.097528	-9.593056	1.251200
-61.821637	-7.700841	1.256205
-62.692101	-3.125331	1.261210
-62.893051	-11.810544	1.266214
-62.667328	-12.309835	1.271219
-62.644721	-4.285060	1.276224
-62.934356	-10.169646	1.281229
-63.299209	-7.788937	1.286234
-63.948808	-13.711388	1.291238
-64.576486	3.997829	1.296243
-64.448261	-4.300669	1.301248
-64.447630	-13.435638	1.306253
-64.645928	-0.587584	1.311258
-64.324289	-9.739410	1.316262
-65.037478	-4.890200	1.321267
-65.512166	-10.128263	1.326272
-65.750475	-8.189027	1.331277
-65.911569	-2.849517	1.336282
-66.090988	-10.620700	1.341286
-66.700547	3.280552	1.346291
-67.115614	-9.576725	1.351296
-67.290659	5.406567	1.356301
-67.611364	-8.316448	1.361306
-67.570583	-15.695097	1.366310
-67.688793	-5.713145	1.371315
-67.705136	-13.718336	1.376320
-67.577583	-19.406008	1.381325
-68.284198	-8.531160	1.386330
-68.791525	-16.671903	1.391334
-68.891979	-9.961704	1.396339
-69.122153	-9.802569	1.401344
-69.432574	-9.083139	1.406349
-70.138954	-10.048864	1.411354
-70.504611	-7.386034	1.416358
-70.953191	-8.088590	1.421363
-70.728889	-8.049323	1.426368
-70.820435	-3.337205	1.431373
-71.010955	-8.332055	1.436378
-70.870739	-17.561179	1.441382
-70.961052	0.928088	1.446387
-71.291707	-8.884119	1.451392
-71.987392	-4.646577	1.456397
-72.128796	-4.543387	1.461402
-72.318836	-11.219983	1.466406
-72.630438	-0.081796	1.471411
-73.464815	-5.393093	1.476416
-73.878364	-3.919545	1.481421
-73.970683	-4.739318	1.486426
-74.218698	-0.530137	1.491430
-74.208233	0.981324	1.496435
-73.922584	-1.564561	1.501440
-74.070782	4.044938	1.506445
-74.152296	-1.332244	1.511450
-74.370091	0.836843	1.516454
-75.473881	0.436583	1.521459
-75.267467	1.705629	1.526464
-75.512609	3.162928	1.531469
-76.193135	2.020848	1.536474
-76.577470	-1.802112	1.541478
-77.058401	2.150436	1.546483
-76.887556	-5.916544	1.551488
-77.130890	-5.598943	1.556493
-77.297929	-2.093442	1.561498
-77.116766	-15.894831	1.566502
-77.553780	-1.844166	1.571507
-77.840208	-2.010983	1.576512
-78.437544	-6.566287	1.581517
-78.709981	2.405810	1.586522
-78.621917	-9.241081	1.591526
-78.727408	-12.133424	1.596531
-79.085538	-3.284087	1.601536
-80.082418	-3.731258	1.606541
-80.474691	-4.134511	1.611546
-80.090095	-4.304324	1.616550
-80.257049	-0.603478	1.621555
-80.202619	-1.843404	1.626560
-80.073308	-0.949544	1.631565
-81.359779	-6.135446	1.636570
-81.747945	-7.328511	1.641574
-82.123184	-6.394303	1.646579
-82.183174	-3.825509	1.651584
-81.988014	-9.784465	1.656589
-81.976595	-1.096972	1.661594
-82.064386	-11.007809	1.666598
-82.255314	-3.230053	1.671603
-82.814679	-5.901200	1.676608
-83.205979	-6.173387	1.681613
-83.602018	-5.009986	1.686618
-83.613447	-17.265344	1.691622
-83.740982	-3.037229	1.696627
-84.335526	-6.362429	1.701632
-84.879643	-12.650440	1.706637
-85.022881	-1.450748	1.711642
-85.086524	-9.309776	1.716646
-85.285837	-15.643447	1.721651
-85.271691	-17.794493	1.726656
-85.734215	-19.023785	1.731661
-86.374325	-8.859100	1.736666
-86.581052	-17.048440	1.741670
-86.839119	-14.183601	1.746675
-86.890678	-15.444452	1.751680
-86.612370	-20.313298	1.756685
-87.039625	-13.988238	1.761690
-87.400405	-13.229880	1.766694
-88.024184	-6.725057	1.771699
-88.069191	-11.847210	1.776704
-88.317773	-16.326479	1.781709
-88.783896	-15.282499	1.786714
-88.700407	-16.491915	1.791718
-88.983891	-12.150964	1.796723
-89.195800	-15.676680	1.801728
-89.559043	-15.330536	1.806733
-90.171466	-7.820411	1.811738
-90.162758	-16.739844	1.816742
-90.392597	-14.808523	1.821747
-90.405220	-16.951583	1.826752
-90.358064	-16.753133	1.831757
-91.052296	-16.514179	1.836762
-91.655279	-19.787065	1.841766
-91.918796	-15.357465	1.846771
-91.719278	-16.760737	1.851776
-91.593939	-17.524206	1.856781
-91.969332	-13.129751	1.861786
-92.290655	-14.667377	1.866790
-93.030920	-8.207987	1.871795
-93.211378	-19.148148	1.876800
-93.133416	-9.753392	1.881805
-93.511077	0.956869	1.886810
-93.984604	-16.134743	1.891814
-94.380918	-14.516248	1.896819
-94.789258	-15.428718	1.901824
-94.916159	-25.777064	1.906829
-95.271537	-8.913145	1.911834
-94.970441	-21.827846	1.916838
-94.995097	-12.123254	1.921843
-94.920054	-15.867189	1.926848
-94.986680	-21.115799	1.931853
-95.684181	-16.533809	1.936858
-96.171864	-18.552999	1.941862
-96.847070	-16.453786	1.946867
-97.489909	-21.564929	1.951872
-96.872685	-19.539670	1.956877
-97.774722	-23.046195	1.961882
-97.819755	-21.738664	1.966886
-98.360602	-12.160514	1.971891
-98.107486	-17.519703	1.976896
-97.995818	-22.160854	1.981901
-97.832358	-16.834256	1.986906
-98.264143	-18.609723	1.991910
-99.244076	-14.548482	1.996915
-99.488426	-18.249216	2.006912
-99.223421	-21.836498	2.016909
-98.436696	-20.528285	2.026906
-98.376935	-18.119647	2.036902
-97.448447	-14.208416	2.046899
-96.777011	-22.029289	2.056896
-96.691036	-23.213924	2.066893
-96.301436	-20.564132	2.076890
-95.291212	-19.953066	2.086886
-95.352295	-17.950208	2.096883
-94.494980	-17.111292	2.106880
-93.870008	-13.337299	2.116877
-93.795394	-18.724660	2.126874
-93.153631	-13.535184	2.136870
-92.698641	-16.595755	2.146867
-92.018959	-14.184082	2.156864
-91.158444	-14.009580	2.166861
-91.159234	-14.485532	2.176858
-90.836640	-17.391596	2.186854
-89.950135	-20.142099	2.196851
-89.573897	-23.757682	2.206848
-89.074249	-25.093619	2.216845
-88.295154	-15.348253	2.226842
-88.034507	-16.782521	2.236838
-87.621740	-14.356278	2.246835
-86.645934	-19.386684	2.256832
-86.130660	-14.329978	2.266829
-86.406741	-15.879259	2.276826
-85.712498	-17.905976	2.286822
-85.083929	-16.656330	2.296819
-84.697240	-9.555055	2.306816
-83.564878	-11.019692	2.316813
-83.427321	-14.896075	2.326810
-83.302459	-13.602718	2.336806
-82.517184	-5.189102	2.346803
-81.649213	-8.247140	2.356800
-81.641940	-12.945634	2.366797
-81.330934	-10.736674	2.376794
-80.566535	-11.921048	2.386790
-80.184015	-21.507109	2.396787
-79.347243	-16.602046	2.406784
-78.976959	-17.236272	2.416781
-78.568340	-9.130154	2.426778
-77.559642	-9.243573	2.436774
-77.482933	-12.039956	2.446771
-77.313399	-15.121021	2.456768
-76.393253	-12.461684	2.466765
-76.108789	-9.030018	2.476762
-75.788145	-8.618504	2.486758
-74.865420	-11.454433	2.496755
-74.471351	-15.497779	2.506752
-73.880949	-13.908681	2.516749
-73.016515	-10.260094	2.526746
-73.109415	-8.341472	2.536742
-72.772904	-7.343189	2.546739
-72.162546	-15.196823	2.556736
-71.416764	-9.534359	2.566733
-71.172507	-8.797812	2.576730
-69.834422	-7.521434	2.586726
-69.762898	-8.532173	2.596723
-69.620501	-13.328722	2.606720
-69.389451	-11.442018	2.616717
-68.503618	-11.405272	2.626714
-68.305672	-9.558134	2.636710
-67.413890	-8.294975	2.646707
-66.741392	-7.951810	2.656704
-66.685473	-3.222093	2.666701
-65.893780	-8.251447	2.676698
-65.416278	-9.499148	2.686694
-65.266595	-6.785708	2.696691
-64.074663	-7.501281	2.706688
-63.829230	-3.413686	2.716685
-63.943887	-0.512820	2.726682
-62.655958	-7.569783	2.736678
-62.142652	-6.136454	2.746675
-62.115811	-4.030000	2.756672
-61.830075	-5.046776	2.766669
-60.644729	-6.617987	2.776666
-60.523292	3.086746	2.786662
-60.089951	-3.173492	2.796659
-59.039120	-2.686507	2.806656
-58.913799	-2.061655	2.816653
-58.728219	-6.404392	2.826650
-57.780756	-9.167950	2.836646
-57.308496	-6.914760	2.846643
-57.265745	-16.763258	2.856640
-56.398149	-17.776222	2.866637
-55.844426	-8.801245	2.876634
-55.671710	-10.913880	2.886630
-54.804281	-11.662448	2.896627
-54.169072	-13.583358	2.906624
-54.084601	-7.020828	2.916621
-53.660362	-6.819312	2.926618
-52.754806	-9.039683	2.936614
-52.666091	-2.829556	2.946611
-51.712500	-8.112549	2.956608
-51.323502	-3.433053	2.966605
-50.928633	-8.286829	2.976602
-50.362204	-8.302297	2.986598
-49.624609	-7.996188	2.996595
-49.523996	-12.776136	3.006592
-49.271982	-13.191212	3.016589
-48.411913	-9.453576	3.026586
-48.010811	-10.950423	3.036582
-47.365548	-13.675192	3.046579
-46.699795	-10.666868	3.056576
-46.636233	-5.355144	3.066573
-45.833462	-8.160928	3.076570
-44.867854	-10.805579	3.086566
-44.596213	-1.934439	3.096563
-44.746878	-8.133521	3.106560
-44.086005	-8.268361	3.116557
-43.570290	-5.921597	3.126554
-43.319310	-9.233890	3.136550
-42.087994	-12.783620	3.146547
-41.929873	-13.548679	3.156544
-41.589923	-8.072301	3.166541
-40.643459	-11.415207	3.176538
-40.362750	-8.917097	3.186534
-40.205572	-8.251681	3.196531
-39.072835	-9.833141	3.206528
-38.884234	-3.687964	3.216525
-38.849004	-4.054690	3.226522
-37.838978	-3.902566	3.236518
-37.266904	-14.323801	3.246515
-36.894437	-6.612587	3.256512
-36.060626	-10.964477	3.266509
-35.746643	-12.819343	3.276506
-35.514822	-11.390766	3.286502
-34.969883	-11.387657	3.296499
-33.832343	-10.278999	3.306496
-33.753448	-5.803821	3.316493
-33.533061	-11.352453	3.326490
-33.252680	-3.862299	3.336486
-32.705523	-2.093540	3.346483
-31.713920	-8.190948	3.356480
-30.682317	-9.325514	3.366477
-31.055111	-12.232396	3.376474
-30.668449	-5.859405	3.386470
-29.838452	-11.102561	3.396467
-29.368634	-9.189600	3.406464
-29.098447	-7.031964	3.416461
-28.015907	-10.480192	3.426458
-27.559620	-7.566987	3.436454
-27.248048	-6.382198	3.446451
-27.260258	-9.065262	3.456448
-26.431090	-7.270494	3.466445
-25.938018	-9.552363	3.476442
-25.659905	-8.201001	3.486438
-24.619421	-6.744324	3.496435
-24.178267	-4.235638	3.506432
-24.034580	-6.772620	3.516429
-23.146690	-6.613308	3.526426
-22.991877	-7.457049	3.536422
-22.595970	-10.585285	3.546419
-21.426702	-6.889758	3.556416
-21.143396	-8.917371	3.566413
-21.128840	-4.820187	3.576410
-20.164136	-1.723844	3.586406
-19.406938	-1.814962	3.596403
-19.431540	-8.750181	3.606400
-19.230690	-2.900444	3.616397
-18.336874	-6.564793	3.626394
-17.888581	-6.211165	3.636390
-17.448340	-9.649048	3.646387
-16.416594	-7.668704	3.656384
-16.318821	-8.117116	3.666381
-16.350736	-2.692761	3.676378
-15.313457	-5.888683	3.686374
-14.747081	-5.643523	3.696371
-14.371977	-7.928774	3.706368
-13.329061	-4.933110	3.716365
-13.080900	-5.825900	3.726362
-13.222498	-0.539275	3.736358
-12.577202	-3.112895	3.746355
-12.126980	-7.899567	3.756352
-11.246029	-3.208275	3.766349
-10.296328	-1.924464	3.776346
-10.151850	-1.804056	3.786342
-9.841222	-8.417602	3.796339
-9.718242	-8.988344	3.806336
-8.613179	-7.993444	3.816333
-8.428308	-12.136896	3.826330
-7.723714	-12.090277	3.836326
-7.020462	-3.608128	3.846323
-6.703783	-14.903072	3.856320
-6.475204	-10.421464	3.866317
-5.921210	-5.444258	3.876314
-5.436366	-5.726188	3.886310
-4.961550	-9.362244	3.896307
-3.920792	-4.609095	3.906304
-3.802753	1.033064	3.916301
-3.680412	6.554380	3.926298
-3.339578	14.327161	3.936294
-2.849415	28.709549	3.946291
-2.246287	44.344710	3.956288
-1.795729	59.243458	3.966285
-1.480170	79.407925	3.976282
-0.876424	97.632406	3.986278
-0.484608	119.012890	3.996275
0.000000	130.023026	4.001280
0.024403	155.788353	4.006285
0.107238	162.982136	4.011290
0.876079	160.411859	4.016294
0.247783	168.158533	4.021299
0.666422	167.161978	4.026304
0.379948	166.862947	4.031309
0.670142	178.066184	4.036314
1.026113	189.280243	4.041318
1.035675	201.111713	4.046323
1.039398	193.358635	4.051328
1.182020	205.807835	4.056333
1.364186	199.552973	4.061338
1.255922	187.686244	4.066342
0.865469	185.836013	4.071347
1.010417	165.050452	4.076352
0.993183	176.909627	4.081357
0.979745	181.420610	4.086362
0.895365	180.968724	4.091366
1.001615	200.606346	4.096371
1.490721	201.462542	4.101376
1.194677	205.759258	4.106381
0.905232	203.890916	4.111386
1.158519	203.926178	4.116390
1.224097	206.918415	4.121395
1.008005	199.333950	4.126400
1.363539	205.460989	4.131405
1.086484	204.947078	4.136410
1.076778	204.761266	4.141414
1.113484	208.690496	4.146419
1.349753	206.078955	4.151424
0.963452	207.841638	4.156429
1.217272	211.861210	4.161434
1.292474	206.341570	4.166438
0.982434	211.717858	4.171443
1.025992	203.668884	4.176448
1.128755	203.990542	4.181453
1.025935	203.682804	4.186458
1.201914	205.205555	4.191462
1.089378	207.797886	4.196467
1.261836	207.626899	4.201472
1.596695	221.120544	4.206477
1.705989	225.285217	4.211482
1.498648	210.829259	4.216486
1.017168	210.485559	4.221491
1.605677	209.923425	4.226496
1.306030	214.566866	4.231501
1.068662	224.842803	4.236506
1.836000	226.152777	4.241510
1.759626	227.306072	4.246515
2.006315	214.657899	4.251520
1.498649	208.943120	4.256525
1.144683	204.519906	4.261530
1.272077	198.830403	4.266534
1.480914	212.544613	4.271539
1.775686	227.676273	4.276544
1.154851	222.195524	4.281549
1.467548	229.653788	4.286554
1.626938	242.893530	4.291558
1.331661	237.401289	4.296563
1.690239	235.723015	4.301568
1.660573	230.320190	4.306573
1.522571	238.592512	4.311578
1.580047	235.651423	4.316582
1.327877	239.601267	4.321587
1.862125	240.429468	4.326592
1.756898	233.864416	4.331597
1.769551	234.624084	4.336602
1.704090	241.285186	4.341606
1.840527	241.063332	4.346611
1.914294	237.079586	4.351616
1.717141	241.050512	4.356621
1.615581	248.097269	4.361626
1.726976	233.744204	4.366630
1.648624	249.075613	4.371635
2.109938	240.609536	4.376640
1.754155	239.577828	4.381645
1.831614	240.862334	4.386650
1.938029	241.082944	4.391654
1.540673	246.494030	4.396659
1.832936	237.313770	4.401664
1.982431	246.059057	4.406669
1.654088	236.355621	4.411674
2.038639	246.760255	4.416678
1.864406	247.951267	4.421683
1.834985	236.745346	4.426688
1.373764	235.414770	4.431693
1.698790	243.681852	4.436698
2.076072	246.250105	4.441702
2.014800	265.094239	4.446707
1.976990	242.000210	4.451712
2.017854	250.171680	4.456717
1.994043	251.870392	4.461722
2.375425	263.881876	4.466726
1.889894	255.297306	4.471731
2.172578	248.170524	4.476736
1.955740	241.715121	4.481741
1.708833	252.065472	4.486746
2.021542	256.631396	4.491750
2.196771	264.083237	4.496755
2.329812	269.645864	4.501760
2.470787	276.606096	4.506765
2.174902	259.573929	4.511770
1.967092	246.785504	4.516774
1.675498	262.867779	4.521779
2.478812	264.302435	4.526784
2.190053	278.643162	4.531789
2.357326	282.176639	4.536794
2.408638	281.866266	4.541798
2.141038	275.968836	4.546803
2.445764	267.393895	4.551808
2.415137	261.848939	4.556813
2.112576	257.487646	4.561818
2.394660	253.507483	4.566822
2.359358	252.809086	4.571827
2.158746	238.700483	4.576832
2.385101	258.459384	4.581837
2.326671	257.981096	4.586842
2.644933	265.316898	4.591846
2.158689	252.698504	4.596851
2.404070	245.867590	4.601856
2.034942	255.789246	4.606861
2.090865	270.856111	4.611866
2.459629	263.968645	4.616870
2.084401	278.660346	4.621875
2.192040	285.332663	4.626880
2.635341	271.256717	4.631885
2.257745	266.852790	4.636890
2.612542	275.699469	4.641894
2.500870	279.537255	4.646899
2.311023	277.868889	4.651904
2.428991	275.600163	4.656909
2.463704	282.550171	4.661914
2.481886	272.057605	4.666918
2.386403	274.688959	4.671923
2.733949	270.241711	4.676928
2.242414	268.833665	4.681933
2.277005	269.259954	4.686938
2.418500	272.555369	4.691942
2.216078	279.398222	4.696947
2.502499	284.821000	4.701952
2.863655	294.894463	4.706957
2.490391	304.053142	4.711962
2.640147	298.346678	4.716966
3.124917	301.308193	4.721971
2.866542	303.794449	4.726976
2.469349	286.272663	4.731981
2.917265	301.624917	4.736986
2.654734	290.281535	4.741990
2.713658	289.939117	4.746995
2.785728	300.987346	4.752000
2.710183	300.245290	4.757005
2.845256	299.535055	4.762010
3.246764	300.224018	4.767014
2.494958	293.826793	4.772019
2.327374	279.830493	4.777024
2.684139	287.930922	4.782029
2.928494	305.337415	4.787034
2.764762	295.408162	4.792038
2.769652	302.818767	4.797043
2.981379	295.543675	4.802048
2.916319	302.555207	4.807053
2.587959	298.306512	4.812058
2.889398	302.701055	4.817062
2.764705	306.780176	4.822067
2.863372	294.780034	4.827072
2.930047	300.265651	4.832077
2.832954	292.876135	4.837082
3.219248	296.170879	4.842086
2.525137	300.434280	4.847091
2.381337	300.878074	4.852096
2.281052	307.590162	4.857101
2.441070	324.352131	4.862106
2.958396	333.574495	4.867110
2.829325	334.702189	4.872115
2.891904	331.697089	4.877120
3.180044	325.572432	4.882125
2.788752	339.682339	4.887130
3.055458	337.280439	4.892134
3.203919	333.537284	4.897139
3.170310	327.718698	4.902144
3.196926	331.921561	4.907149
2.800090	334.623352	4.912154
2.983573	322.223349	4.917158
2.816884	329.233370	4.922163
2.938547	341.813038	4.927168
3.527412	355.098381	4.932173
3.074339	358.985619	4.937178
3.310155	356.106539	4.942182
3.503677	355.331171	4.947187
3.160063	343.843111	4.952192
3.111665	357.556436	4.957197
3.231629	358.653942	4.962202
3.459229	357.999423	4.967206
3.298364	363.533399	4.972211
3.255377	359.143892	4.977216
3.303505	360.464050	4.982221
3.398327	369.305684	4.987226
3.621935	358.406863	4.992230
3.236008	363.109431	4.997235
3.292450	356.943210	5.002240
3.525123	361.700812	5.007245
3.373126	350.284026	5.012250
3.501420	358.247880	5.017254
3.383377	356.084138	5.022259
3.330939	353.555903	5.027264
3.515041	362.900562	5.032269
3.554524	353.038655	5.037274
3.830154	356.925990	5.042278
3.299136	349.524240	5.047283
3.478574	346.767769	5.052288
3.662481	361.838591	5.057293
3.316339	356.096811	5.062298
3.746006	357.252749	5.067302
3.671832	356.987032	5.072307
3.354489	346.906765	5.077312
3.256418	348.346446	5.082317
3.503135	359.619769	5.087322
3.882166	355.392444	5.092326
3.473581	365.031012	5.097331
3.727003	361.993513	5.102336
3.455553	363.202409	5.107341
3.536379	368.651370	5.112346
3.798800	359.006120	5.117350
3.776436	358.511990	5.122355
3.818485	352.110955	5.127360
3.551475	359.691332	5.132365
3.473710	369.020750	5.137370
3.786813	361.175703	5.142374
3.691203	367.192415	5.147379
3.618311	362.428971	5.152384
3.906988	359.966003	5.157389
3.672750	363.256368	5.162394
3.716046	356.882555	5.167398
3.520657	358.816501	5.172403
3.837257	360.049181	5.177408
3.754925	360.324533	5.182413
3.373451	361.472319	5.187418
3.502956	359.935371	5.192422
3.210438	363.355171	5.197427
3.781314	376.424072	5.202432
3.631170	389.353085	5.207437
3.557697	388.664752	5.212442
4.039878	387.247002	5.217446
3.962507	400.132200	5.222451
3.809757	394.966180	5.227456
4.148519	397.124851	5.232461
3.521223	397.905648	5.237466
4.034981	395.606292	5.242470
3.776997	400.691634	5.247475
3.968794	392.308193	5.252480
3.795642	388.344183	5.257485
3.878680	398.427460	5.262490
4.223949	391.046341	5.267494
3.970988	398.423717	5.272499
4.107274	400.349906	5.277504
3.926665	392.988777	5.282509
3.936667	394.888912	5.287514
4.504344	396.196248	5.292518
4.097234	402.000717	5.297523
3.913742	395.492563	5.302528
4.153189	399.572779	5.307533
4.269951	397.855598	5.312538
4.475014	393.973010	5.317542
4.530944	399.764934	5.322547
4.441165	396.946869	5.327552
4.274137	398.398764	5.332557
4.199792	397.752410	5.337562
4.377968	395.631962	5.342566
4.170328	400.152277	5.347571
4.262574	397.245262	5.352576
4.571464	394.187521	5.357581
4.165773	408.064450	5.362586
4.419471	396.303976	5.367590
4.322930	397.021744	5.372595
4.173279	400.898016	5.377600
4.377055	399.922623	5.382605
4.475316	404.194155	5.387610
4.412465	397.634843	5.392614
4.362746	399.610977	5.397619
4.276729	401.316060	5.402624
4.294329	400.969826	5.407629
4.045339	406.165571	5.412634
4.560729	398.520654	5.417638
4.365088	396.041978	5.422643
4.401138	391.063936	5.427648
4.445566	387.127832	5.432653
4.407785	400.088173	5.437658
4.299785	398.042742	5.442662
4.444189	404.920175	5.447667
4.476977	394.021749	5.452672
4.503226	397.183931	5.457677
4.427187	403.897768	5.462682
4.582338	393.533204	5.467686
4.179184	402.289388	5.472691
4.543637	395.872241	5.477696
4.367963	404.992338	5.482701
4.524021	425.202170	5.487706
4.801272	413.536451	5.492710
4.618375	422.738466	5.497715
4.471784	426.129969	5.502720
4.908835	422.811431	5.507725
4.767207	425.392237	5.512730
4.525903	424.370764	5.517734
4.601567	425.502448	5.522739
4.534168	423.916996	5.527744
4.818325	421.274795	5.532749
4.669977	427.647973	5.537754
4.868639	418.769247	5.542758
4.657147	426.569177	5.547763
4.572753	430.606925	5.552768
4.561623	423.634099	5.557773
4.347712	438.296473	5.562778
4.768977	427.266202	5.567782
4.684700	438.155514	5.572787
4.631274	424.982220	5.577792
4.697199	425.214867	5.582797
4.134075	434.508468	5.587802
4.617977	423.776069	5.592806
4.633211	449.378626	5.597811
4.747470	452.093679	5.602816
4.847414	457.968914	5.607821
4.470680	459.598810	5.612826
4.832982	454.524490	5.617830
4.822913	460.639555	5.622835
4.941650	455.291406	5.627840
4.836129	457.476495	5.632845
4.970491	464.554929	5.637850
5.230953	460.755899	5.642854
4.991808	467.007572	5.647859
4.990011	461.546770	5.652864
5.041901	458.125847	5.657869
4.883402	461.031115	5.662874
4.952616	451.169157	5.667878
5.277943	462.823029	5.672883
5.020787	456.108791	5.677888
5.218472	461.807998	5.682893
5.178609	462.269908	5.687898
4.865336	453.365626	5.692902
4.859549	464.492579	5.697907
5.104891	457.407802	5.702912
5.187067	466.243692	5.707917
5.217339	461.392289	5.712922
5.368468	461.277127	5.717926
5.030571	467.956998	5.722931
5.308449	456.620107	5.727936
5.136961	455.563981	5.732941
5.112463	455.746875	5.737946
4.980085	453.895512	5.742950
4.968299	461.973196	5.747955
5.049139	462.929973	5.752960
5.287278	467.396615	5.757965
5.345852	477.170030	5.762970
5.156346	474.660329	5.767974
4.975491	486.517828	5.772979
5.009422	485.389202	5.777984
5.370424	489.954303	5.782989
5.022679	494.622565	5.787994
5.651197	490.329814	5.792998
5.791303	489.344831	5.798003
5.435773	499.098625	5.803008
5.542111	486.341848	5.808013
5.453059	505.742239	5.813018
5.239668	498.209672	5.818022
5.271804	495.007901	5.823027
5.426153	495.763852	5.828032
5.549171	500.223914	5.833037
5.121458	500.183098	5.838042
5.828440	490.737856	5.843046
5.278585	497.812392	5.848051
5.551757	490.411195	5.853056
5.840123	493.855206	5.858061
5.453165	497.555108	5.863066
5.599143	494.063342	5.868070
5.564150	498.007480	5.873075
5.580601	493.331816	5.878080
5.676001	487.243948	5.883085
5.589029	500.297176	5.888090
5.670634	496.261152	5.893094
6.056426	500.328014	5.898099
5.808323	495.229848	5.903104
5.772457	478.452757	5.908109
5.518511	481.888494	5.913114
5.576183	465.554739	5.918118
5.326232	482.106917	5.923123
5.261480	494.081557	5.928128
5.891236	494.303321	5.933133
5.420275	498.768010	5.938138
5.422824	497.266873	5.943142
5.359959	492.005224	5.948147
5.465979	491.549623	5.953152
5.585317	498.390004	5.958157
5.220347	496.251148	5.963162
5.537830	508.928965	5.968166
5.927421	532.796230	5.973171
5.971289	525.556721	5.978176
5.994552	528.132341	5.983181
5.781669	539.316336	5.988186
6.265458	528.763660	5.993190
6.183145	511.755641	5.998195
5.789458	505.203707	6.003200
5.615365	495.634014	6.008205
5.516951	510.689375	6.013210
5.910618	515.921605	6.018214
5.933701	536.339891	6.023219
5.896425	537.354123	6.028224
6.056738	532.270602	6.033229
5.752136	530.352434	6.038234
6.077703	528.547379	6.043238
5.699873	516.817787	6.048243
5.666423	514.910368	6.053248
6.013683	524.004717	6.058253
5.955533	530.768138	6.063258
6.047266	522.568937	6.068262
5.874526	525.964003	6.073267
5.764448	519.076983	6.078272
5.536103	513.754914	6.083277
5.741109	532.004503	6.088282
5.982120	533.718593	6.093286
5.625813	531.549880	6.098291
5.904155	531.332347	6.103296
6.030975	535.783304	6.108301
5.971933	537.507813	6.113306
6.227358	532.399858	6.118310
5.961888	537.321114	6.123315
6.044929	530.470585	6.128320
6.202374	514.077236	6.133325
5.605058	510.954441	6.138330
5.989963	501.348613	6.143334
5.981376	505.856913	6.148339
5.645537	497.915214	6.153344
5.565320	500.096513	6.158349
5.725294	522.681194	6.163354
6.319321	520.811948	6.168358
5.898598	529.664849	6.173363
6.176704	519.582163	6.178368
5.830092	510.711786	6.183373
5.698559	502.787757	6.188378
5.701642	500.796538	6.193382
5.976469	522.836094	6.198387
5.796288	517.698453	6.203392
5.696752	523.911834	6.208397
5.882519	523.069660	6.213402
6.185220	512.142635	6.218406
5.961875	516.175789	6.223411
5.984089	505.006313	6.228416
5.898843	498.192547	6.233421
5.655919	503.138672	6.238426
5.838768	500.968496	6.243430
5.703132	519.708232	6.248435
6.096293	525.067439	6.253440
6.319446	517.101242	6.258445
5.784524	516.561151	6.263450
6.199091	502.906337	6.268454
5.600973	504.193416	6.273459
5.622360	510.889784	6.278464
5.676926	505.969222	6.283469
5.684749	515.005912	6.288474
5.810260	517.925530	6.293478
5.982025	542.132982	6.298483
5.869932	537.341836	6.303488
6.061021	535.145425	6.308493
6.015887	530.813059	6.313498
5.587275	516.159413	6.318502
5.492940	514.172879	6.323507
5.880368	525.343690	6.328512
5.874001	525.529898	6.333517
6.047610	530.011191	6.338522
6.069943	526.647640	6.343526
5.840963	536.663485	6.348531
5.962494	528.680761	6.353536
5.996189	529.186733	6.358541
6.060009	534.207974	6.363546
6.076942	516.662143	6.368550
5.500132	507.388441	6.373555
5.537992	519.155872	6.378560
5.825817	525.655581	6.383565
5.765825	529.459217	6.388570
6.517148	531.107743	6.393574
5.948698	530.890920	6.398579
5.731046	518.630402	6.403584
6.375254	526.670332	6.408589
5.864174	521.634059	6.413594
5.908474	508.947922	6.418598
6.004910	503.525303	6.423603
5.615675	505.244695	6.428608
5.866930	505.813900	6.433613
5.600553	503.165171	6.438618
5.939118	513.614108	6.443622
5.952186	524.606554	6.448627
5.761791	521.207190	6.453632
6.004246	515.622052	6.458637
6.149357	519.194578	6.463642
6.106334	504.634961	6.468646
5.873205	499.851635	6.473651
5.697576	496.761824	6.478656
5.639043	498.674901	6.483661
5.653390	501.660681	6.488666
5.845197	518.504228	6.493670
5.812114	532.652673	6.498675
5.870205	537.087582	6.503680
6.439077	532.120718	6.508685
6.054505	520.382768	6.513690
6.267737	500.931698	6.518694
5.992750	500.784286	6.523699
5.852444	500.721924	6.528704
5.844664	504.007773	6.533709
5.572132	503.018896	6.538714
6.029278	503.121043	6.543718
5.955733	496.470513	6.548723
5.788690	502.415040	6.553728
6.165701	491.671681	6.558733
5.951529	494.266288	6.563738
6.150805	496.278360	6.568742
6.180337	497.342109	6.573747
6.076143	498.792291	6.578752
5.722279	502.506645	6.583757
5.764586	514.884298	6.588762
6.051663	495.042510	6.593766
5.749847	501.043495	6.598771
6.018362	503.574747	6.603776
6.074572	498.081434	6.608781
5.668810	508.227574	6.613786
5.933751	503.075822	6.618790
5.891129	497.174795	6.623795
5.861525	502.537698	6.628800
5.602074	496.425313	6.633805
5.539288	514.685285	6.638810
5.631941	499.659586	6.643814
6.035177	501.256230	6.648819
5.602872	500.502793	6.653824
5.606397	497.841338	6.658829
5.695296	500.964553	6.663834
5.778494	499.625298	6.668838
5.916564	495.337394	6.673843
5.941406	502.547254	6.678848
5.762933	508.559587	6.683853
5.781209	506.550460	6.688858
6.124391	509.044878	6.693862
5.521758	511.103511	6.698867
5.703388	517.168895	6.703872
6.046872	526.554355	6.708877
5.980073	533.323551	6.713882
6.253568	519.683796	6.718886
5.822095	510.641381	6.723891
5.627287	505.302513	6.728896
5.848532	503.739110	6.733901
5.910639	526.050309	6.738906
6.126199	521.600969	6.743910
5.773734	509.138211	6.748915
5.955796	514.230049	6.753920
5.922025	507.376772	6.758925
5.703172	509.078210	6.763930
5.855922	497.881597	6.768934
5.922843	511.301463	6.773939
5.718587	503.984651	6.778944
5.833252	510.238332	6.783949
5.796323	520.310573	6.788954
6.111737	526.540490	6.793958
5.973446	527.898243	6.798963
5.817175	522.313614	6.803968
5.679332	512.768890	6.808973
5.665477	526.536438	6.813978
5.708816	536.392138	6.818982
5.753602	537.345221	6.823987
5.857170	537.091903	6.828992
6.206549	530.515774	6.833997
5.926916	541.563215	6.839002
6.020503	542.055323	6.844006
6.367280	537.187201	6.849011
5.920824	525.287218	6.854016
6.018554	504.167230	6.859021
5.694240	507.197253	6.864026
5.859110	497.443551	6.869030
5.763992	508.784838	6.874035
5.764214	505.696295	6.879040
5.747043	516.821026	6.884045
5.501445	533.487390	6.889050
5.955371	525.368714	6.894054
6.167119	535.320256	6.899059
6.125942	535.855204	6.904064
6.207107	517.789993	6.909069
5.553778	512.638353	6.914074
5.868597	496.767565	6.919078
5.735580	515.371882	6.924083
5.797141	524.455131	6.929088
6.010168	528.633493	6.934093
5.924454	529.239359	6.939098
5.950337	526.886782	6.944102
5.791279	522.330161	6.949107
5.756568	527.125384	6.954112
6.505146	524.306207	6.959117
6.070054	513.718038	6.964122
5.972029	505.500935	6.969126
5.893721	500.955024	6.974131
5.894191	496.533811	6.979136
6.078493	497.593439	6.984141
5.491568	506.201522	6.989146
5.609303	503.011821	6.994150
5.959459	510.913557	6.999155
5.791584	502.783406	7.004160
6.089154	503.144248	7.009165
5.777345	501.923095	7.014170
6.089595	499.208739	7.019174
5.881659	500.662484	7.024179
6.181746	495.931364	7.029184
5.988117	499.027955	7.034189
5.539674	503.878266	7.039194
5.595797	498.836282	7.044198
5.974151	500.432704	7.049203
5.655016	496.574145	7.054208
5.790090	497.463137	7.059213
5.858255	496.539204	7.064218
5.655765	498.685891	7.069222
6.139868	518.964463	7.074227
5.730147	514.663073	7.079232
5.743686	515.359658	7.084237
5.881959	529.930644	7.089242
5.552651	539.249920	7.094246
6.108760	537.006876	7.099251
5.920504	536.434635	7.104256
6.183044	532.684777	7.109261
5.893096	521.981988	7.114266
5.694212	508.122092	7.119270
5.999424	518.628456	7.124275
6.241286	523.206981	7.129280
6.050400	504.577060	7.134285
5.791149	511.897908	7.139290
6.020546	513.956105	7.144294
5.908950	508.091953	7.149299
5.548592	503.755750	7.154304
6.165885	496.346505	7.159309
5.980946	505.445698	7.164314
6.038017	506.314060	7.169318
6.009731	509.681452	7.174323
5.975570	510.766603	7.179328
5.919090	499.027026	7.184333
5.722460	508.268465	7.189338
5.878582	506.338337	7.194342
5.514735	494.829834	7.199347
5.213811	504.273054	7.204352
5.713833	513.209092	7.209357
5.907768	530.662079	7.214362
6.017882	525.920376	7.219366
6.227302	537.163102	7.224371
5.590459	515.976679	7.229376
6.043377	520.888685	7.234381
5.553910	520.485519	7.239386
5.900773	525.710111	7.244390
6.038505	527.683439	7.249395
6.187784	536.121867	7.254400
5.962704	517.226645	7.259405
5.962149	513.080294	7.264410
6.049634	506.523469	7.269414
5.970279	507.399425	7.274419
5.853493	506.842978	7.279424
5.775452	504.129118	7.284429
5.509147	502.010430	7.289434
5.765759	502.769180	7.294438
5.981067	511.479447	7.299443
5.995134	518.404365	7.304448
5.884434	507.668548	7.309453
6.033916	511.326586	7.314458
6.170505	511.518523	7.319462
5.979166	504.116688	7.324467
5.879264	506.412548	7.329472
5.963009	503.287085	7.334477
5.779820	514.846418	7.339482
5.799092	503.021080	7.344486
5.606959	503.533664	7.349491
5.756651	506.873161	7.354496
5.913702	498.424375	7.359501
5.710887	504.578283	7.364506
5.967185	497.826953	7.369510
6.215932	503.473317	7.374515
5.985310	502.240299	7.379520
5.945310	495.241041	7.384525
6.009773	499.286915	7.389530
6.385249	496.940191	7.394534
5.913382	499.900122	7.399539
5.428536	497.928925	7.404544
5.700782	498.959387	7.409549
6.309911	505.837065	7.414554
6.197303	505.659014	7.419558
6.064545	503.744362	7.424563
5.649319	504.268828	7.429568
6.056007	501.593298	7.434573
5.713007	505.778875	7.439578
5.670212	505.890798	7.444582
6.055738	503.648971	7.449587
5.969799	505.873844	7.454592
5.875479	498.433647	7.459597
5.563667	502.967691	7.464602
5.440021	508.332750	7.469606
5.955326	500.183991	7.474611
5.788224	506.537614	7.479616
6.053002	497.480550	7.484621
5.376829	505.217360	7.489626
5.716084	502.798092	7.494630
5.694491	505.607681	7.499635
6.010672	522.816434	7.504640
6.279153	514.218548	7.509645
5.854429	517.313747	7.514650
5.720653	508.954361	7.519654
5.392937	516.180775	7.524659
5.802153	532.037553	7.529664
6.315907	531.351823	7.534669
6.061437	522.481375	7.539674
6.180887	506.151161	7.544678
6.175272	508.713207	7.549683
5.963801	508.173031	7.554688
6.266097	497.858821	7.559693
5.843505	513.059631	7.564698
5.705867	512.467958	7.569702
6.051767	502.219540	7.574707
5.623774	501.642205	7.579712
6.086718	493.918308	7.584717
5.760210	511.452525	7.589722
5.764087	502.827224	7.594726
5.986284	505.252874	7.599731
5.729652	507.328409	7.604736
5.860502	500.880243	7.609741
5.991602	501.400869	7.614746
5.829285	511.367375	7.619750
5.871568	503.972043	7.624755
5.689511	506.468585	7.629760
5.887190	499.719265	7.634765
5.641529	509.771007	7.639770
5.948986	505.054254	7.644774
5.937838	502.261433	7.649779
5.631936	519.245419	7.654784
6.032342	508.836414	7.659789
5.834524	514.766506	7.664794
5.838410	516.669642	7.669798
5.741752	518.203236	7.674803
5.983773	504.968516	7.679808
6.136494	506.915283	7.684813
5.794461	511.552609	7.689818
5.856946	508.052762	7.694822
5.958105	502.822359	7.699827
5.974453	505.971403	7.704832
6.278967	503.159855	7.709837
6.035990	510.421766	7.714842
5.859852	505.546908	7.719846
5.872737	513.622901	7.724851
5.685947	505.080877	7.729856
5.879215	502.777350	7.734861
5.738066	506.867339	7.739866
5.961287	501.671189	7.744870
5.756628	511.896511	7.749875
5.572657	509.307150	7.754880
5.704908	503.929909	7.759885
5.516322	518.875294	7.764890
5.609402	523.649748	7.769894
5.910623	530.617302	7.774899
5.718491	543.906832	7.779904
5.913539	531.558620	7.784909
5.897684	547.718273	7.789914
5.954950	548.293358	7.794918
5.734966	543.080996	7.799923
5.701010	543.536997	7.804928
6.370663	542.414588	7.809933
6.005134	548.787273	7.814938
6.126009	536.367669	7.819942
6.216078	519.826022	7.824947
5.702089	514.407790	7.829952
5.507411	510.788512	7.834957
5.839421	524.777821	7.839962
5.944649	523.287305	7.844966
5.969875	516.179356	7.849971
6.007050	515.245557	7.854976
6.159772	509.203640	7.859981
5.838479	505.739324	7.864986
6.129161	508.229806	7.869990
6.020760	510.623375	7.874995
5.829024	512.129890	7.880000
6.112438	502.950347	7.885005
5.913887	507.434457	7.890010
5.895789	517.089363	7.895014
5.976491	511.865502	7.900019
5.617826	513.270404	7.905024
5.841602	508.511858	7.910029
5.809556	513.102192	7.915034
5.758184	503.845674	7.920038
5.893395	513.472427	7.925043
5.701681	511.112077	7.930048
6.099058	507.847650	7.935053
5.610371	520.959526	7.940058
5.679306	512.160642	7.945062
5.593973	498.451465	7.950067
5.348197	522.414853	7.955072
6.381322	524.227668	7.960077
5.810316	535.551481	7.965082
5.833660	531.933785	7.970086
6.013480	541.061990	7.975091
5.852414	546.257035	7.980096
6.126408	543.363310	7.985101
6.112644	535.907979	7.990106
5.817840	520.740992	7.995110
5.769255	505.345972	8.000115
5.617315	512.565654	8.005133
6.084503	512.577109	8.010150
5.643872	526.433755	8.015168
5.985119	540.407767	8.020186
6.158142	536.174547	8.025203
5.944611	530.654062	8.030221
6.008076	513.649772	8.035238
5.680067	509.822538	8.040256
5.796657	507.923498	8.045274
6.145437	508.254145	8.050291
5.684757	520.302233	8.055309
5.821787	521.529104	8.060326
5.880813	536.743067	8.065344
6.159988	540.563533	8.070362
6.068229	548.430179	8.075379
5.644782	545.489937	8.080397
5.620156	538.953592	8.085414
5.925587	545.054191	8.090432
5.712213	544.396121	8.095450
6.201710	546.934014	8.100467
5.911043	550.579970	8.105485
5.842081	547.166685	8.110502
6.157202	542.410755	8.115520
6.149091	544.947790	8.120538
6.313978	547.624276	8.125555
6.130962	547.811313	8.130573
6.286021	543.710781	8.135590
5.705461	541.736648	8.140608
5.851382	540.647254	8.145626
6.324605	539.163527	8.150643
5.914860	554.339003	8.155661
6.290785	542.857541	8.160678
6.340116	545.674807	8.165696
6.013437	540.150616	8.170714
5.982193	523.246836	8.175731
5.802728	538.766025	8.180749
6.088558	535.690219	8.185766
6.279583	549.432245	8.190784
6.303518	545.795717	8.195802
6.074320	521.313067	8.200819
5.763145	529.582153	8.205837
6.081024	533.713901	8.210854
6.386928	540.374616	8.215872
6.255545	533.071953	8.220890
5.976651	526.208259	8.225907
5.525214	518.199015	8.230925
6.200995	529.743581	8.235942
6.434330	541.518303	8.240960
6.145599	547.646436	8.245978
6.285571	536.769956	8.250995
5.987977	538.801622	8.256013
6.307589	538.713116	8.261030
6.445221	536.161029	8.266048
5.984226	520.961764	8.271066
6.454546	517.503862	8.276083
6.099941	515.734816	8.281101
6.079957	505.350363	8.286118
6.306032	515.058509	8.291136
5.935890	511.656724	8.296154
6.084546	508.016085	8.301171
6.038971	522.065948	8.306189
6.260184	530.218921	8.311206
6.395306	536.250089	8.316224
6.248128	533.760127	8.321242
6.447668	512.612739	8.326259
6.276248	517.535891	8.331277
6.325276	505.833807	8.336294
6.337383	506.735326	8.341312
6.159486	515.418719	8.346330
6.153948	508.321590	8.351347
6.403032	512.484014	8.356365
6.013352	508.412288	8.361382
6.133028	508.210445	8.366400
6.180191	510.806230	8.371418
6.175701	503.076102	8.376435
5.927844	518.655805	8.381453
6.405015	533.815874	8.386470
6.381703	545.682310	8.391488
6.431841	546.319875	8.396506
6.398614	540.385894	8.401523
6.507265	521.837019	8.406541
6.022487	507.301107	8.411558
6.318701	520.357430	8.416576
6.205950	533.263002	8.421594
6.198571	538.195213	8.426611
6.235301	545.127653	8.431629
6.110512	545.041879	8.436646
6.565929	552.055174	8.441664
6.092151	559.410326	8.446682
6.494837	542.436241	8.451699
6.368137	553.212796	8.456717
6.625094	539.712797	8.461734
6.352974	548.077584	8.466752
6.397102	547.624885	8.471770
6.633750	543.226216	8.476787
6.403313	546.750394	8.481805
6.437692	534.938518	8.486822
6.261712	518.091583	8.491840
6.435984	543.194992	8.496858
6.516613	540.654115	8.501875
6.149621	536.301281	8.506893
6.584845	539.495752	8.511910
6.610498	538.673108	8.516928
6.148421	533.080600	8.521946
6.465678	538.791865	8.526963
6.429735	542.071251	8.531981
6.296244	541.469042	8.536998
6.530558	544.749339	8.542016
5.894282	550.713389	8.547034
6.565305	538.559681	8.552051
6.531909	552.321158	8.557069
6.817016	548.430568	8.562087
6.506259	545.229556	8.567104
6.473007	550.806561	8.572122
6.638648	538.001952	8.577139
6.540965	550.700332	8.582157
6.519151	545.320129	8.587175
6.640855	549.693801	8.592192
6.202611	543.997547	8.597210
6.472409	542.588252	8.602227
6.520594	541.405012	8.607245
6.933551	539.780488	8.612263
6.480024	535.570913	8.617280
6.103785	536.943801	8.622298
6.542666	539.694588	8.627315
6.243142	547.518480	8.632333
6.373727	555.325083	8.637351
6.541320	544.024171	8.642368
6.475099	548.248662	8.647386
6.450214	538.279339	8.652403
6.375040	542.685023	8.657421
6.467887	539.795101	8.662439
6.372873	546.539138	8.667456
5.987550	542.875509	8.672474
6.081965	540.478402	8.677491
6.257530	552.787465	8.682509
6.811561	574.816441	8.687527
7.095423	573.768175	8.692544
6.416193	573.431129	8.697562
6.684293	570.134647	8.702579
6.689180	575.602793	8.707597
6.798537	573.191199	8.712615
6.675847	565.781971	8.717632
6.449373	563.301592	8.722650
6.618571	565.501416	8.727667
6.752974	570.392444	8.732685
6.462748	577.192441	8.737703
6.689058	569.019758	8.742720
6.733871	574.221074	8.747738
6.494187	571.041159	8.752755
6.410149	567.846492	8.757773
6.260500	568.144335	8.762791
6.235177	568.399347	8.767808
6.463974	575.258856	8.772826
6.754148	568.470775	8.777843
6.520932	578.435715	8.782861
6.497901	576.173004	8.787879
6.772465	570.412238	8.792896
6.443219	576.423675	8.797914
6.699400	590.549408	8.802931
6.742491	603.139092	8.807949
6.721055	605.470878	8.812967
6.874524	608.877561	8.817984
6.875033	612.056050	8.823002
6.826052	598.126578	8.828019
6.783599	583.227601	8.833037
6.362799	592.527206	8.838055
6.739137	599.541021	8.843072
6.732267	606.571058	8.848090
7.139448	614.972590	8.853107
7.076681	615.556616	8.858125
6.591194	611.014737	8.863143
6.783833	614.982023	8.868160
6.544904	617.033313	8.873178
6.643062	615.975445	8.878195
6.805685	611.886633	8.883213
6.660747	610.462750	8.888231
6.843962	602.578466	8.893248
6.582136	615.103308	8.898266
6.974260	611.265251	8.903283
6.653830	613.480421	8.908301
6.850523	614.810403	8.913319
7.392087	609.206970	8.918336
6.904612	609.906600	8.923354
7.179448	611.063416	8.928371
7.211664	607.945743	8.933389
6.733510	610.774393	8.938407
7.377490	605.503583	8.943424
6.789483	604.291055	8.948442
6.820748	606.439323	8.953459
6.905865	604.745863	8.958477
6.722795	605.651562	8.963495
7.159708	603.101277	8.968512
6.618574	609.580857	8.973530
6.863516	612.373418	8.978547
6.610260	606.176657	8.983565
6.841480	617.969700	8.988583
6.821626	608.982110	8.993600
6.891318	615.364672	8.998618
6.608633	608.508458	9.003635
7.031863	612.350359	9.008653
6.484662	607.945660	9.013671
6.749983	607.585454	9.018688
7.065966	624.787719	9.023706
7.181937	630.520541	9.028723
7.006775	621.992098	9.033741
6.905795	635.224129	9.038759
7.354963	624.623528	9.043776
7.055154	622.042299	9.048794
6.861665	614.515253	9.053811
7.250400	619.636601	9.058829
6.840809	624.696466	9.063847
7.217760	614.850891	9.068864
7.103715	625.572058	9.073882
6.845067	619.897803	9.078899
7.087650	625.308495	9.083917
7.208054	637.388981	9.088935
7.282107	636.527413	9.093952
6.946842	629.670055	9.098970
6.801641	635.337671	9.103987
6.875925	641.772040	9.109005
7.019916	649.343808	9.114023
7.259972	637.233834	9.119040
7.212019	641.822427	9.124058
7.216865	645.758422	9.129075
7.245518	645.808249	9.134093
7.377564	642.480546	9.139111
7.351655	644.259965	9.144128
7.230355	630.920158	9.149146
7.267301	619.042639	9.154163
7.104785	616.847309	9.159181
7.082715	615.041686	9.164199
7.212878	620.302304	9.169216
7.170958	634.868952	9.174234
7.156897	639.410202	9.179251
7.348006	645.377420	9.184269
7.060003	632.237451	9.189287
7.337297	633.812732	9.194304
7.504489	647.338136	9.199322
7.302224	619.010965	9.204339
7.140252	615.035351	9.209357
7.172906	618.901384	9.214375
7.285119	614.713446	9.219392
7.153481	619.586936	9.224410
6.920920	632.701787	9.229427
7.260293	637.728369	9.234445
7.011569	646.014733	9.239463
7.508671	639.265380	9.244480
7.389565	645.227478	9.249498
7.418246	644.917679	9.254515
7.573322	641.747372	9.259533
7.027551	641.867129	9.264551
7.252252	640.912902	9.269568
7.432327	643.842777	9.274586
6.899747	642.458677	9.279603
7.327528	643.548636	9.284621
7.141937	646.997894	9.289639
7.522571	642.088772	9.294656
7.574459	641.987320	9.299674
7.222491	636.855446	9.304691
7.125820	641.010797	9.309709
7.003793	644.706599	9.314727
7.278835	645.231142	9.319744
7.422678	639.006794	9.324762
7.287120	639.941632	9.329779
7.473516	634.249377	9.334797
7.077092	640.390853	9.339815
7.231374	642.247709	9.344832
7.261874	640.775087	9.349850
7.228644	640.262168	9.354867
7.215575	644.894194	9.359885
7.571804	662.939978	9.364903
7.618291	651.903517	9.369920
7.645655	642.753767	9.374938
7.231862	639.838875	9.379955
7.719831	631.314384	9.384973
7.596041	638.000041	9.389991
7.659518	641.690318	9.395008
7.748917	650.081310	9.400026
7.225384	642.635872	9.405043
7.379424	641.672481	9.410061
7.219757	641.533430	9.415079
7.309783	633.041179	9.420096
7.524981	644.574511	9.425114
7.418192	662.784170	9.430131
7.644109	667.000076	9.435149
7.438544	672.031878	9.440167
7.946759	668.523576	9.445184
7.683921	653.581111	9.450202
7.331472	653.638344	9.455219
7.606365	644.512952	9.460237
7.410816	652.215157	9.465255
7.538934	667.903209	9.470272
7.853333	673.168963	9.475290
7.400329	668.799826	9.480307
7.671469	665.998458	9.485325
7.842963	668.864015	9.490343
7.933761	660.794822	9.495360
7.805983	649.623057	9.500378
7.739061	651.084881	9.505395
7.659974	644.847451	9.510413
7.510735	645.479654	9.515431
7.306402	642.271627	9.520448
7.329714	648.503233	9.525466
7.286728	662.135302	9.530483
7.910863	663.354349	9.535501
7.690654	670.497888	9.540519
7.756030	668.125451	9.545536
7.592789	667.664374	9.550554
7.617148	669.440590	9.555571
7.787229	670.624600	9.560589
7.850929	672.064795	9.565607
7.772698	666.124243	9.570624
7.892624	666.501650	9.575642
7.480548	682.336256	9.580659
7.869859	672.247275	9.585677
7.997961	671.071460	9.590695
7.589312	664.823444	9.595712
7.588362	660.015299	9.600730
7.696191	674.897715	9.605747
7.865418	668.769342	9.610765
7.962868	675.159537	9.615783
7.874375	666.603135	9.620800
8.033622	666.356747	9.625818
7.732858	655.660447	9.630835
7.735270	650.857259	9.635853
7.545062	651.422629	9.640871
7.805664	662.038279	9.645888
7.942575	663.129363	9.650906
7.929325	675.683164	9.655923
8.156866	673.614559	9.660941
7.744452	647.895987	9.665959
7.522977	658.234009	9.670976
7.869953	658.434850	9.675994
7.657072	671.047294	9.681011
7.801210	668.517729	9.686029
7.857318	670.307583	9.691047
7.884051	676.773264	9.696064
8.331983	667.411146	9.701082
8.274467	679.795520	9.706099
8.123947	650.182442	9.711117
7.854850	647.590021	9.716135
7.643026	633.744764	9.721152
7.885030	641.947105	9.726170
8.237985	664.637813	9.731187
7.801702	654.689892	9.736205
8.122475	653.166444	9.741223
7.746058	649.705632	9.746240
7.633884	649.943927	9.751258
7.787517	676.685903	9.756275
8.360430	663.102571	9.761293
7.923760	670.310694	9.766311
7.999327	671.617042	9.771328
8.288723	667.604066	9.776346
7.893871	675.184769	9.781363
8.079828	672.390421	9.786381
8.339555	670.629064	9.791399
7.496479	663.924678	9.796416
7.716692	674.232084	9.801434
7.808234	674.915354	9.806451
8.114333	670.450034	9.811469
8.221827	672.138078	9.816487
8.468040	676.514001	9.821504
8.217876	670.090535	9.826522
8.253747	674.819774	9.831539
8.097675	671.462813	9.836557
8.076507	674.343742	9.841575
7.971936	674.853203	9.846592
8.163813	680.295931	9.851610
7.733681	673.455445	9.856627
8.358594	673.179184	9.861645
7.857115	677.247063	9.866663
7.609559	678.664397	9.871680
8.249700	672.523390	9.876698
8.313308	678.246398	9.881715
8.359711	677.532902	9.886733
8.082235	675.525881	9.891751
8.082519	677.133261	9.896768
7.943241	667.452663	9.901786
8.163795	679.475655	9.906803
7.799252	683.197257	9.911821
7.969243	676.232193	9.916839
7.577182	687.233483	9.921856
8.165867	685.124755	9.926874
8.482011	700.493926	9.931891
8.132889	688.180515	9.936909
8.089742	687.716872	9.941927
7.930516	700.291716	9.946944
8.330332	696.276589	9.951962
8.529923	706.602391	9.956979
8.676224	698.566898	9.961997
8.819435	691.388166	9.967015
8.179566	685.575257	9.972032
8.373349	671.560245	9.977050
8.157335	676.809906	9.982067
8.323498	674.369993	9.987085
8.445766	672.473536	9.992103
8.150830	677.483133	9.997120
8.091855	676.144609	10.002138
8.005324	682.143646	10.007155
8.207218	690.253843	10.012173
8.433644	696.886451	10.017191
8.048921	697.086421	10.022208
8.261192	692.661434	10.027226
8.318638	695.292750	10.032243
8.190984	700.502197	10.037261
8.385251	697.225789	10.042279
8.110076	705.753951	10.047296
8.741919	702.946778	10.052314
8.377985	698.096375	10.057331
8.735147	698.799435	10.062349
8.215165	699.991036	10.067367
8.202385	703.546917	10.072384
8.633171	697.220898	10.077402
8.412319	703.108338	10.082419
8.247242	706.066250	10.087437
8.441750	699.237265	10.092455
8.312505	702.077046	10.097472
8.567995	697.177607	10.102490
8.313091	708.451455	10.107507
8.223840	703.592962	10.112525
8.708415	705.313835	10.117543
8.240403	702.330946	10.122560
8.440432	698.290638	10.127578
8.303220	692.808241	10.132595
8.307065	701.446878	10.137613
8.444396	717.836561	10.142631
8.251267	730.475309	10.147648
8.863619	726.607644	10.152666
8.640185	734.494221	10.157683
8.864044	727.807992	10.162701
8.718495	719.023622	10.167719
8.721103	712.328766	10.172736
8.674753	707.795824	10.177754
8.541110	715.706496	10.182771
8.276156	707.791067	10.187789
8.582527	712.476310	10.192807
8.648564	731.407974	10.197824
8.617262	732.117888	10.202842
9.095719	727.813762	10.207859
8.458866	717.429752	10.212877
8.866429	698.492211	10.217895
8.640567	707.507846	10.222912
8.499207	702.253284	10.227930
8.666658	707.741403	10.232947
8.629980	722.650945	10.237965
8.808872	722.594599	10.242983
8.712266	726.330106	10.248000
8.974100	719.467917	10.253018
8.426439	720.531433	10.258035
8.909414	731.688618	10.263053
9.032759	717.008104	10.268071
8.732243	719.316442	10.273088
8.564767	707.106785	10.278106
8.661336	708.777352	10.283123
8.630465	726.041697	10.288141
8.934105	721.481893	10.293159
8.557030	729.212425	10.298176
8.958113	733.156444	10.303194
8.850435	737.097317	10.308211
8.638060	733.326070	10.313229
9.229150	732.040510	10.318247
8.798699	718.669347	10.323264
8.897225	713.231757	10.328282
8.445719	716.149315	10.333299
8.728733	714.160095	10.338317
9.082482	725.452841	10.343335
8.914275	734.426663	10.348352
8.960756	732.641168	10.353370
9.039669	734.294978	10.358387
8.672041	746.193390	10.363405
8.781623	730.697475	10.368423
8.703415	739.060762	10.373440
8.951064	737.438792	10.378458
9.171008	732.860564	10.383475
8.735899	735.469916	10.388493
8.921412	724.745793	10.393511
8.943244	732.900002	10.398528
9.245362	732.239820	10.403546
8.650041	736.683075	10.408563
8.822142	731.620674	10.413581
9.161342	730.541778	10.418599
9.160551	736.327044	10.423616
9.197412	732.226745	10.428634
9.026046	741.525878	10.433651
8.822334	743.429235	10.438669
9.104376	742.276738	10.443687
8.998203	739.476426	10.448704
8.947827	733.395023	10.453722
8.776663	742.068570	10.458739
8.608601	734.890580	10.463757
8.860935	733.817408	10.468775
8.630192	733.975345	10.473792
8.964670	728.260896	10.478810
9.119351	731.428050	10.483827
8.396662	731.918226	10.488845
9.045803	746.559898	10.493863
9.020474	771.041060	10.498880
8.816709	765.697210	10.503898
8.859724	762.469062	10.508915
9.026762	774.956869	10.513933
9.234175	769.290216	10.518951
9.101473	772.906915	10.523968
9.015970	778.939283	10.528986
9.302985	765.472101	10.534003
9.238366	772.365524	10.539021
8.953026	760.603271	10.544039
9.151570	778.891039	10.549056
9.105867	776.244871	10.554074
9.197979	763.954782	10.559091
8.969090	770.863597	10.564109
8.887646	774.252136	10.569127
8.667828	772.198155	10.574144
8.648074	780.904127	10.579162
8.964816	792.820338	10.584179
8.930595	808.148823	10.589197
9.070126	801.448182	10.594215
9.143915	808.317914	10.599232
9.287993	808.111042	10.604250
9.315384	801.788401	10.609267
9.382972	807.218294	10.614285
9.419696	800.139818	10.619303
9.147185	803.991476	10.624320
8.877721	806.095483	10.629338
9.497446	810.499743	10.634355
9.632780	804.104504	10.639373
9.561461	810.633326	10.644391
9.463840	813.038386	10.649408
9.380070	803.699279	10.654426
9.245629	797.203056	10.659443
9.374150	808.140268	10.664461
9.634563	799.606718	10.669479
9.766400	803.928394	10.674496
9.652475	811.597674	10.679514
9.701026	807.948545	10.684531
9.334752	807.915946	10.689549
9.672583	804.451183	10.694567
9.631990	800.117644	10.699584
9.099985	806.774326	10.704602
9.324217	808.128503	10.709619
9.309945	809.483990	10.714637
9.561139	810.140041	10.719655
9.501506	805.018752	10.724672
9.243038	807.986637	10.729690
9.550690	807.547571	10.734707
9.517874	803.858771	10.739725
9.772281	801.557366	10.744743
9.804972	800.589062	10.749760
9.411846	805.868884	10.754778
9.429549	795.742154	10.759795
9.436607	802.382003	10.764813
9.502736	803.648588	10.769831
9.338654	812.427295	10.774848
9.510002	800.857480	10.779866
9.950118	804.619472	10.784883
9.481191	809.708315	10.789901
9.792334	807.804579	10.794919
9.726198	802.975690	10.799936
9.457503	809.967488	10.804954
9.867908	803.934155	10.809971
9.694476	814.451322	10.814989
9.545007	803.000377	10.820007
9.785383	809.212243	10.825024
9.795640	809.730643	10.830042
9.673823	814.698624	10.835059
9.427406	811.516821	10.840077
9.789245	812.149038	10.845095
9.431309	808.403845	10.850112
9.677125	818.165012	10.855130
9.816192	800.057987	10.860147
9.784268	806.490132	10.865165
9.845191	808.953183	10.870183
9.663636	809.151004	10.875200
10.068792	815.850911	10.880218
9.878859	806.754567	10.885235
9.550199	807.091310	10.890253
9.808425	802.190991	10.895271
9.766918	813.581537	10.900288
9.555848	809.744311	10.905306
9.750973	806.125237	10.910323
9.629778	809.832553	10.915341
9.633659	812.044436	10.920359
9.423225	815.210263	10.925376
10.089001	832.377864	10.930394
10.036685	833.695955	10.935411
9.660680	826.736206	10.940429
10.050668	830.926168	10.945447
9.732629	822.497846	10.950464
9.920527	825.368590	10.955482
10.402753	823.007803	10.960499
10.018616	817.533577	10.965517
9.925470	810.607698	10.970535
10.340049	794.428176	10.975552
9.709109	795.792086	10.980570
9.968446	795.263389	10.985587
9.983309	807.605172	10.990605
9.752973	802.046036	10.995623
9.783853	805.733680	11.000640
9.501542	814.554799	11.005658
9.998401	829.536318	11.010675
9.928308	830.384149	11.015693
9.769663	835.385006	11.020711
9.797329	832.469605	11.025728
9.837914	840.572343	11.030746
10.059419	831.720826	11.035763
9.779632	834.166685	11.040781
9.556553	835.778395	11.045799
9.777038	835.799408	11.050816
10.013119	846.608606	11.055834
9.893576	838.570216	11.060851
10.038483	853.043535	11.065869
10.212674	867.123062	11.070887
10.328912	874.046026	11.075904
10.402180	860.673210	11.080922
10.406723	847.541302	11.085939
10.139372	842.617382	11.090957
10.078376	837.967542	11.095975
9.974499	839.971301	11.100992
9.892468	842.018291	11.106010
10.095791	835.221644	11.111027
10.205565	859.267995	11.116045
10.323147	861.287049	11.121063
10.150918	856.276904	11.126080
10.320754	854.967005	11.131098
10.212068	838.445765	11.136115
9.990151	850.404768	11.141133
10.356260	857.951272	11.146151
10.396567	858.510365	11.151168
10.619284	862.481592	11.156186
10.259003	840.299160	11.161203
10.241934	840.156374	11.166221
10.183564	842.042761	11.171239
10.064221	844.536851	11.176256
10.171698	869.196558	11.181274
10.255004	867.063235	11.186291
10.387375	870.256552	11.191309
9.908742	863.282288	11.196327
10.118000	862.787864	11.201344
10.182353	872.800758	11.206362
10.359312	874.719828	11.211379
10.335880	873.382880	11.216397
10.238463	869.423673	11.221415
10.462815	871.872663	11.226432
10.398795	867.024901	11.231450
10.828466	858.891614	11.236467
10.738340	867.785263	11.241485
10.505995	866.543538	11.246503
10.975214	867.321352	11.251520
10.400896	871.799748	11.256538
10.628087	876.321390	11.261555
10.938452	874.961448	11.266573
10.483937	854.705134	11.271591
10.451546	834.119114	11.276608
10.124404	853.503418	11.281626
10.621224	862.492376	11.286643
10.621953	865.019339	11.291661
10.458982	869.881560	11.296679
10.575295	870.319017	11.301696
10.488966	874.096161	11.306714
10.551838	873.924783	11.311731
10.627535	867.705920	11.316749
10.470041	874.467926	11.321767
10.610779	869.127224	11.326784
10.543277	867.642070	11.331802
10.767065	871.583203	11.336819
10.715217	869.324630	11.341837
10.740248	873.588820	11.346855
10.793595	872.234827	11.351872
10.521200	872.721300	11.356890
10.488713	873.631801	11.361907
10.686295	870.436299	11.366925
10.571804	866.852736	11.371943
10.647102	865.699429	11.376960
10.587226	876.879295	11.381978
10.863441	873.724705	11.386995
10.535973	878.623618	11.392013
10.488776	874.416736	11.397031
10.589746	870.377435	11.402048
10.494628	877.273199	11.407066
10.483705	872.917404	11.412083
10.569860	872.522496	11.417101
10.624782	876.110904	11.422119
10.555055	876.723650	11.427136
10.414612	884.417829	11.432154
10.785268	896.231102	11.437171
10.671606	899.676969	11.442189
11.015076	904.881298	11.447207
11.086486	898.466293	11.452224
10.771033	909.379465	11.457242
10.955599	903.598443	11.462259
11.096808	904.554981	11.467277
10.760653	895.210766	11.472295
11.258625	890.027423	11.477312
10.722620	883.298858	11.482330
10.725532	875.188599	11.487347
11.056308	883.055124	11.492365
10.543020	887.476963	11.497383
11.039847	899.644129	11.502400
10.770043	899.709328	11.507418
10.952264	900.666554	11.512435
10.851461	900.562436	11.517453
10.655045	904.156253	11.522471
11.207012	901.928781	11.527488
11.124422	901.953529	11.532506
11.013956	905.017391	11.537523
11.021945	905.785370	11.542541
11.178502	906.114200	11.547559
11.398722	904.946733	11.552576
11.175617	914.560034	11.557594
10.842691	909.883948	11.562611
10.827741	901.749075	11.567629
11.219148	902.837400	11.572647
11.303115	900.340594	11.577664
11.217914	908.463410	11.582682
10.872918	909.326850	11.587699
11.146481	908.917048	11.592717
10.900227	912.178585	11.597735
11.151890	902.566165	11.602752
11.134810	908.176249	11.607770
10.987956	909.012388	11.612787
11.145302	901.454071	11.617805
10.902686	905.257892	11.622823
11.005775	908.842268	11.627840
11.107404	907.308632	11.632858
11.068359	905.409334	11.637875
11.314682	908.031060	11.642893
10.949800	907.157720	11.647911
11.128539	903.194897	11.652928
11.049427	906.234670	11.657946
11.444903	910.717826	11.662963
10.957785	898.111366	11.667981
11.068436	917.326406	11.672999
11.436457	927.715798	11.678016
11.092639	944.958591	11.683034
11.359703	940.375255	11.688051
11.443534	940.633456	11.693069
11.295758	948.284394	11.698087
11.754025	943.035172	11.703104
11.356052	939.717423	11.708122
11.700221	935.898055	11.713139
11.691949	917.327128	11.718157
11.220611	922.875046	11.723175
11.502507	909.202692	11.728192
11.393411	906.048914	11.733210
11.050239	905.104659	11.738227
11.666768	914.044691	11.743245
11.513650	915.766865	11.748263
11.595251	909.207260	11.753280
11.090068	907.400901	11.758298
11.068820	914.865130	11.763315
11.521895	923.535400	11.768333
11.484178	927.908416	11.773351
11.511150	937.836600	11.778368
11.595852	939.961893	11.783386
11.708145	933.745211	11.788403
11.846142	937.337985	11.793421
11.456000	938.089223	11.798439
11.361968	941.747193	11.803456
11.407849	926.210847	11.808474
11.350823	931.159869	11.813491
11.146748	929.148139	11.818509
11.364433	938.515240	11.823527
11.338815	938.260094	11.828544
11.411168	941.888149	11.833562
11.606269	941.177574	11.838579
11.737768	931.353157	11.843597
11.426489	949.643273	11.848615
11.607845	938.210275	11.853632
11.644092	934.722200	11.858650
11.514469	935.263769	11.863667
11.609423	943.527234	11.868685
11.512115	968.718233	11.873703
11.947141	959.487206	11.878720
11.980265	959.138084	11.883738
11.468168	966.211202	11.888755
11.858524	959.652413	11.893773
11.509661	964.779689	11.898791
11.955809	953.993350	11.903808
12.054705	965.206039	11.908826
11.681067	977.597333	11.913843
11.892112	971.531992	11.918861
11.914725	971.492471	11.923879
11.840669	968.146272	11.928896
12.171093	971.452082	11.933914
11.556455	953.203169	11.938931
11.954367	942.844098	11.943949
12.154236	954.667195	11.948967
11.819911	944.140811	11.953984
11.843565	938.063997	11.959002
11.622636	951.389779	11.964019
11.922459	957.719413	11.969037
12.067384	964.519169	11.974055
11.795170	969.508168	11.979072
12.384390	961.512573	11.984090
12.001400	955.886933	11.989107
12.051875	947.412870	11.994125
11.852527	950.665860	11.999143
11.950314	963.877460	12.004160
12.159535	953.245705	12.009178
11.977189	964.836449	12.014195
12.042471	961.971091	12.019213
11.833520	965.114656	12.024231
11.898494	962.078098	12.029248
11.993327	966.700422	12.034266
11.823653	969.289477	12.039283
12.489716	961.498470	12.044301
12.025151	959.330670	12.049319
12.304090	960.656905	12.054336
12.196625	970.645561	12.059354
11.945100	967.868884	12.064371
12.071200	963.676585	12.069389
12.035580	968.058319	12.074407
12.047371	975.495060	12.079424
12.110986	963.682740	12.084442
12.103915	967.192856	12.089459
12.254586	965.605819	12.094477
12.526375	964.698694	12.099495
12.433540	961.763068	12.104512
12.121586	959.084585	12.109530
11.950586	959.539703	12.114547
12.051639	953.144174	12.119565
12.222933	965.242471	12.124583
11.879819	964.527721	12.129600
12.012051	956.779057	12.134618
12.105711	965.409266	12.139635
12.341054	958.539155	12.144653
12.373869	963.438666	12.149671
12.241777	968.676496	12.154688
12.571325	963.111196	12.159706
12.260693	967.354622	12.164723
12.577294	959.099856	12.169741
12.435819	965.168335	12.174759
12.489685	968.765601	12.179776
12.455469	960.185088	12.184794
12.013747	961.329497	12.189811
12.480594	971.762394	12.194829
12.510013	984.993994	12.199847
12.459444	981.115579	12.204864
12.278890	970.551903	12.209882
12.491004	988.997900	12.214899
12.590096	985.255718	12.219917
12.357169	995.726169	12.224935
12.378046	1002.142564	12.229952
12.854067	996.766373	12.234970
12.824048	999.035469	12.239987
12.670101	980.980694	12.245005
12.556123	968.651347	12.250023
11.994494	972.378096	12.255040
12.324203	978.040614	12.260058
12.267022	988.641793	12.265075
12.591813	996.977458	12.270093
12.705626	987.819685	12.275111
12.659154	994.623197	12.280128
12.443422	991.151249	12.285146
12.479364	1000.872879	12.290163
12.920846	993.333998	12.295181
12.788330	995.070878	12.300199
12.472399	997.144023	12.305216
12.917688	999.452120	12.310234
12.588409	999.122855	12.315251
12.489125	987.793378	12.320269
12.602865	997.548578	12.325287
12.432264	989.431167	12.330304
12.554419	992.171497	12.335322
12.642622	997.917321	12.340339
12.356868	997.606831	12.345357
12.761741	1004.428516	12.350375
12.537279	1019.600138	12.355392
13.115531	1016.436447	12.360410
12.777937	1025.199520	12.365427
12.772936	1028.759699	12.370445
13.092202	1024.754678	12.375463
12.910135	1024.129785	12.380480
13.074119	1020.218587	12.385498
12.978624	1035.651140	12.390515
12.927912	1030.075956	12.395533
12.916023	1019.853591	12.400551
12.709854	1030.890871	12.405568
13.010030	1022.986022	12.410586
12.937850	1025.719958	12.415603
12.992573	1029.291900	12.420621
13.110051	1021.274399	12.425639
12.917220	1024.849541	12.430656
12.985275	1013.002985	12.435674
13.104794	1018.781818	12.440691
13.129247	1012.450522	12.445709
13.155315	1007.496069	12.450727
13.096906	1017.089639	12.455744
13.337185	1012.939834	12.460762
12.811206	1018.096457	12.465779
12.925289	1014.903730	12.470797
13.050548	1011.986307	12.475815
12.790859	1017.117336	12.480832
13.262771	1014.144082	12.485850
13.107093	1021.336935	12.490867
13.190431	1021.707025	12.495885
13.498858	1018.191575	12.500903
12.951306	1016.198526	12.505920
13.050816	1011.823617	12.510938
13.240037	1018.750702	12.515955
12.845559	1015.549676	12.520973
13.357381	1018.391223	12.525991
12.727782	1021.210774	12.531008
13.213112	1020.534021	12.536026
13.119536	1023.816753	12.541043
12.764324	1022.308366	12.546061
13.228199	1021.314313	12.551079
13.047403	1023.225326	12.556096
12.874200	1043.268991	12.561114
13.255774	1058.942631	12.566131
13.225634	1058.527215	12.571149
13.518816	1060.265258	12.576167
13.233615	1048.918101	12.581184
13.312688	1049.375509	12.586202
13.129648	1058.192531	12.591219
13.492994	1054.640421	12.596237
13.672600	1053.828474	12.601255
13.686649	1057.844149	12.606272
13.769235	1056.804183	12.611290
13.555685	1054.484176	12.616307
13.597671	1050.588449	12.621325
13.678290	1056.989855	12.626343
13.425332	1050.645036	12.631360
13.439285	1043.970599	12.636378
13.352810	1047.329322	12.641395
13.418674	1061.110048	12.646413
13.868027	1055.990212	12.651431
13.517223	1043.975996	12.656448
13.781503	1047.440408	12.661466
13.317218	1049.304279	12.666483
13.483145	1057.745808	12.671501
13.622675	1057.107027	12.676519
13.562908	1060.472354	12.681536
14.041292	1052.475776	12.686554
13.761412	1053.460324	12.691571
13.684675	1062.142033	12.696589
13.694730	1049.900739	12.701607
14.067722	1052.130268	12.706624
13.538611	1029.843245	12.711642
13.813260	1027.157762	12.716659
13.658245	1030.476653	12.721677
13.737360	1015.894124	12.726695
13.649243	1040.542794	12.731712
13.815933	1044.005257	12.736730
13.936279	1055.544368	12.741747
13.594814	1057.741430	12.746765
13.604219	1048.398163	12.751783
13.501136	1061.306114	12.756800
13.574093	1056.371832	12.761818
13.863120	1064.724085	12.766835
13.349349	1054.886765	12.771853
13.676774	1056.048687	12.776871
13.401528	1055.748660	12.781888
13.314468	1052.027052	12.786906
13.642717	1071.697568	12.791923
13.799342	1088.816310	12.796941
13.905991	1084.142179	12.801959
13.727489	1089.904644	12.806976
13.610407	1085.464011	12.811994
13.728641	1092.235567	12.817011
13.819222	1091.829685	12.822029
13.632413	1083.090916	12.827047
13.899862	1097.050488	12.832064
14.187283	1096.045889	12.837082
13.980335	1088.184436	12.842099
13.934840	1086.814510	12.847117
14.164255	1078.413495	12.852135
14.057745	1089.502422	12.857152
13.978485	1087.985337	12.862170
14.266748	1086.024729	12.867187
13.795253	1094.029728	12.872205
13.649072	1087.152271	12.877223
13.824925	1108.916104	12.882240
13.894548	1111.902942	12.887258
14.167731	1115.262355	12.892275
14.063153	1112.908546	12.897293
14.144906	1120.460144	12.902311
14.148849	1128.951764	12.907328
14.308449	1118.937935	12.912346
14.222282	1118.006223	12.917363
14.265496	1118.941208	12.922381
14.272319	1120.519993	12.927399
14.381854	1129.319313	12.932416
14.302198	1123.939432	12.937434
14.682692	1124.365431	12.942451
14.148606	1125.865685	12.947469
14.558155	1121.465781	12.952487
14.223904	1127.708367	12.957504
14.380277	1122.583879	12.962522
14.570662	1125.518438	12.967539
14.302871	1129.216643	12.972557
14.309043	1119.035709	12.977575
14.164677	1125.022055	12.982592
14.212284	1124.718167	12.987610
14.392539	1114.638324	12.992627
14.083469	1126.068683	12.997645
14.290252	1117.223773	13.002663
14.067085	1119.595341	13.007680
14.284040	1119.239395	13.012698
14.420955	1125.113022	13.017715
14.675458	1147.854402	13.022733
14.665702	1143.321966	13.027751
14.516493	1145.810026	13.032768
14.494652	1150.665893	13.037786
14.704358	1152.371314	13.042803
14.503083	1148.978823	13.047821
14.698912	1144.620996	13.052839
14.772193	1160.548541	13.057856
14.643712	1142.784627	13.062874
14.653130	1142.662647	13.067891
14.645988	1146.918067	13.072909
14.780999	1132.094684	13.077927
14.564178	1127.400092	13.082944
14.119624	1137.606481	13.087962
15.033633	1134.975335	13.092979
14.658952	1141.288399	13.097997
14.835604	1143.361092	13.103015
14.498320	1149.737256	13.108032
14.496297	1151.015550	13.113050
14.912942	1147.019568	13.118067
14.598349	1151.838877	13.123085
14.853326	1154.742668	13.128103
14.737648	1151.359229	13.133120
14.614960	1150.948900	13.138138
14.925656	1143.362709	13.143155
14.773310	1150.921593	13.148173
14.762036	1138.812103	13.153191
14.979692	1147.272280	13.158208
14.779163	1148.167318	13.163226
14.992889	1148.242994	13.168243
14.785595	1148.871445	13.173261
14.916017	1138.770706	13.178279
14.799602	1149.889267	13.183296
14.801749	1137.519690	13.188314
14.823839	1150.384547	13.193331
14.867218	1142.783571	13.198349
14.945590	1143.030081	13.203367
14.957886	1152.250621	13.208384
15.109314	1173.422546	13.213402
15.424910	1159.687307	13.218419
15.234612	1155.913875	13.223437
15.334858	1146.602354	13.228455
15.271425	1143.091765	13.233472
15.067535	1148.121867	13.238490
15.497818	1137.804549	13.243507
15.029237	1142.346216	13.248525
15.080802	1146.881275	13.253543
15.245409	1136.929595	13.258560
14.894010	1143.659657	13.263578
15.278159	1136.636877	13.268595
15.205838	1152.329086	13.273613
15.224031	1143.055170	13.278631
15.187629	1141.291228	13.283648
15.009287	1142.348728	13.288666
15.376391	1140.120341	13.293683
15.305042	1147.648488	13.298701
15.290897	1149.129177	13.303719
15.053929	1152.014042	13.308736
15.459719	1166.378706	13.313754
15.899115	1163.288372	13.318771
15.152746	1164.238369	13.323789
15.179030	1148.759375	13.328807
15.009243	1149.283980	13.333824
14.658147	1165.432589	13.338842
15.258456	1165.826912	13.343859
15.568234	1174.291532	13.348877
15.679704	1175.380174	13.353895
15.668577	1175.156088	13.358912
15.721547	1179.792888	13.363930
15.671327	1176.340338	13.368947
15.688548	1179.692154	13.373965
15.883796	1168.567700	13.378983
15.614119	1175.759031	13.384000
15.336610	1182.706787	13.389018
15.773873	1170.419062	13.394035
15.535479	1185.024273	13.399053
15.861293	1171.743222	13.404071
15.634153	1167.066074	13.409088
15.407460	1177.008467	13.414106
16.137579	1167.470585	13.419123
15.347904	1161.376799	13.424141
15.699269	1170.248297	13.429159
15.463706	1169.729892	13.434176
15.483884	1176.249227	13.439194
15.816198	1167.140596	13.444211
15.831427	1165.862179	13.449229
15.824951	1174.844510	13.454247
16.221126	1169.044489	13.459264
15.531108	1166.193938	13.464282
15.860022	1168.292599	13.469299
15.613821	1167.319277	13.474317
15.370766	1160.944034	13.479335
15.681217	1163.609514	13.484352
15.877342	1172.509083	13.489370
15.941390	1160.041838	13.494387
15.867350	1166.867707	13.499405
15.863911	1160.731515	13.504423
15.834690	1171.350629	13.509440
15.712232	1171.228835	13.514458
15.635082	1163.007277	13.519475
15.458003	1169.798638	13.524493
15.661036	1160.583076	13.529511
15.834741	1173.176790	13.534528
15.888551	1177.497319	13.539546
16.212678	1175.377222	13.544563
15.943060	1196.818897	13.549581
16.061741	1191.761650	13.554599
16.142362	1198.480428	13.559616
16.162266	1200.635383	13.564634
16.162810	1193.563114	13.569651
15.890374	1185.813634	13.574669
16.238770	1201.097649	13.579687
15.929449	1196.332136	13.584704
15.845345	1202.471519	13.589722
16.274311	1207.855095	13.594739
16.147397	1198.550059	13.599757
15.924758	1203.305339	13.604775
16.521721	1196.983883	13.609792
15.695155	1197.705832	13.614810
16.298688	1201.505426	13.619827
16.340017	1192.231587	13.624845
15.663208	1192.312218	13.629863
15.958184	1190.063093	13.634880
15.753501	1197.567676	13.639898
15.642322	1207.126403	13.644915
16.225558	1222.557372	13.649933
16.200230	1234.289632	13.654951
16.499787	1221.277447	13.659968
16.094842	1232.329677	13.664986
16.328603	1221.809814	13.670003
16.378950	1233.290178	13.675021
16.468666	1239.614566	13.680039
16.728868	1220.582686	13.685056
16.647804	1226.577092	13.690074
16.717452	1226.659305	13.695091
16.624563	1228.579800	13.700109
16.568340	1221.474400	13.705127
16.639150	1229.675876	13.710144
16.199291	1223.836726	13.715162
16.488024	1226.267631	13.720179
16.428236	1222.651699	13.725197
16.430539	1226.618577	13.730215
16.664345	1222.404829	13.735232
16.569932	1220.898508	13.740250
16.803404	1225.158197	13.745267
16.857554	1220.359258	13.750285
16.513115	1224.823699	13.755303
17.080249	1222.273209	13.760320
16.772322	1219.216858	13.765338
16.780432	1223.944562	13.770355
17.047299	1229.551440	13.775373
16.871318	1232.446693	13.780391
16.879864	1224.404607	13.785408
16.684540	1222.507922	13.790426
16.824577	1222.060777	13.795443
17.094747	1217.564245	13.800461
16.626519	1222.202330	13.805479
16.862804	1222.199470	13.810496
16.482346	1223.556973	13.815514
16.632889	1217.389354	13.820531
17.000874	1224.029061	13.825549
16.728081	1224.146329	13.830567
16.713916	1213.865947	13.835584
16.598155	1214.431606	13.840602
16.875766	1219.374516	13.845619
16.819239	1220.378385	13.850637
16.569802	1226.218787	13.855655
17.191398	1239.622612	13.860672
17.059907	1249.997699	13.865690
17.055484	1249.814627	13.870707
17.194662	1250.032172	13.875725
17.133917	1257.107841	13.880743
17.349876	1237.233291	13.885760
17.038676	1223.838398	13.890778
17.209139	1219.357590	13.895795
17.320081	1222.204145	13.900813
17.084489	1215.352067	13.905831
17.257013	1210.298101	13.910848
16.859522	1215.790981	13.915866
16.828791	1223.599832	13.920883
17.292195	1234.490551	13.925901
17.101285	1245.027438	13.930919
17.310756	1243.268043	13.935936
17.363371	1251.312311	13.940954
17.234602	1248.958944	13.945971
17.305566	1248.003172	13.950989
17.299019	1246.575997	13.956007
17.297667	1235.684834	13.961024
17.312903	1247.462353	13.966042
17.319813	1242.535800	13.971059
17.452820	1248.916013	13.976077
17.072753	1247.129836	13.981095
17.512748	1247.599528	13.986112
17.292767	1251.511492	13.991130
17.314410	1250.075711	13.996147
17.330521	1241.087507	14.001165
17.255188	1244.452696	14.006183
17.392652	1242.168231	14.011200
17.031723	1239.110023	14.016218
17.196740	1243.837340	14.021235
17.473275	1258.697892	14.026253
17.246339	1273.148536	14.031271
17.640225	1272.096375	14.036288
17.792826	1279.702065	14.041306
17.660076	1286.884944	14.046323
17.651341	1288.455299	14.051341
17.579384	1283.836668	14.056359
17.819092	1283.429707	14.061376
17.750900	1277.250257	14.066394
17.456853	1281.525272	14.071411
17.908492	1273.595608	14.076429
17.634474	1285.447039	14.081447
17.988855	1276.690980	14.086464
17.957113	1276.788803	14.091482
17.665979	1278.561035	14.096499
17.809585	1281.312431	14.101517
17.708011	1285.239440	14.106535
17.802628	1277.446060	14.111552
17.954843	1273.527692	14.116570
17.584577	1276.009074	14.121587
18.028822	1269.085730	14.126605
17.801886	1277.798337	14.131623
18.054465	1278.286860	14.136640
17.482277	1278.545044	14.141658
17.576270	1284.444736	14.146675
17.950265	1277.201533	14.151693
17.728124	1279.604844	14.156711
17.993220	1271.963152	14.161728
18.118236	1278.342732	14.166746
17.650594	1279.537909	14.171763
17.896355	1277.927614	14.176781
17.762336	1282.572970	14.181799
17.947323	1292.099634	14.186816
18.162865	1301.858639	14.191834
18.218443	1316.567257	14.196851
18.628791	1301.410723	14.201869
18.310646	1298.854461	14.206887
18.540365	1280.122826	14.211904
18.344136	1283.417887	14.216922
18.175337	1281.166417	14.221939
18.398821	1272.837145	14.226957
18.250670	1280.728066	14.231975
18.677279	1272.484445	14.236992
18.149912	1275.257583	14.242010
18.115583	1280.550193	14.247027
18.232353	1272.972038	14.252045
18.003928	1272.149699	14.257063
17.984038	1268.631477	14.262080
18.520717	1286.417404	14.267098
18.354918	1290.455048	14.272115
18.454638	1285.446578	14.277133
18.604337	1294.902317	14.282151
18.271543	1286.497049	14.287168
18.298171	1287.386761	14.292186
18.605553	1299.491129	14.297203
19.010083	1298.569484	14.302221
18.402047	1295.773440	14.307239
18.347762	1283.500097	14.312256
18.565230	1280.463421	14.317274
18.436888	1292.757652	14.322291
18.696354	1293.011183	14.327309
18.404806	1312.299614	14.332327
18.711006	1297.194581	14.337344
18.979108	1305.397284	14.342362
18.573332	1309.732540	14.347379
19.057223	1304.250614	14.352397
18.538369	1299.859128	14.357415
18.171944	1286.959142	14.362432
18.692969	1305.837815	14.367450
18.566262	1311.194944	14.372467
18.430997	1310.077654	14.377485
18.493448	1316.286118	14.382503
18.464242	1316.046127	14.387520
18.822992	1312.147090	14.392538
18.583658	1315.740629	14.397555
18.978017	1310.470766	14.402573
18.654432	1310.100393	14.407591
18.941542	1310.536744	14.412608
18.982592	1309.971346	14.417626
18.632398	1312.950580	14.422643
18.694503	1312.033278	14.427661
18.472089	1326.321809	14.432679
19.060467	1339.715081	14.437696
19.181665	1341.682419	14.442714
19.129147	1337.884551	14.447731
19.199489	1337.873739	14.452749
19.148523	1334.911818	14.457767
19.564227	1350.204126	14.462784
19.477343	1315.936223	14.467802
18.918943	1306.768715	14.472819
18.892482	1304.601936	14.477837
18.845760	1307.001398	14.482855
18.820004	1330.535503	14.487872
19.426816	1333.526731	14.492890
19.273269	1331.745553	14.497907
19.263436	1335.935329	14.502925
19.354504	1341.169400	14.507943
19.137575	1337.266084	14.512960
19.560012	1332.478955	14.517978
19.450848	1338.342626	14.522995
19.186255	1319.656580	14.528013
19.295500	1321.569992	14.533031
19.441658	1332.566070	14.538048
19.291939	1334.546382	14.543066
19.023219	1347.290665	14.548083
19.490761	1332.480527	14.553101
19.422458	1337.622092	14.558119
19.201655	1334.171378	14.563136
19.346132	1333.373896	14.568154
19.384088	1344.188692	14.573171
19.597293	1338.689374	14.578189
19.641715	1337.158083	14.583207
19.389867	1343.458368	14.588224
19.534236	1340.595198	14.593242
19.423624	1342.596593	14.598259
19.419788	1336.744250	14.603277
19.842014	1337.375939	14.608295
19.365619	1330.793208	14.613312
19.943897	1333.041933	14.618330
19.767307	1337.811676	14.623347
19.725851	1332.230912	14.628365
19.775596	1337.613948	14.633383
19.966260	1337.904070	14.638400
19.857332	1338.948119	14.643418
19.532916	1335.053942	14.648435
19.683961	1334.186082	14.653453
19.585711	1329.886745	14.658471
19.484599	1333.429052	14.663488
19.702074	1332.932468	14.668506
19.407138	1337.912355	14.673523
19.646385	1337.251538	14.678541
19.770809	1352.179493	14.683559
20.019534	1357.236677	14.688576
20.067283	1362.456275	14.693594
19.996199	1376.909947	14.698611
20.222699	1364.014463	14.703629
20.212989	1343.797627	14.708647
19.649034	1336.987272	14.713664
20.225848	1332.850942	14.718682
19.973233	1337.763192	14.723699
20.004288	1352.023159	14.728717
20.067747	1351.923724	14.733735
20.096749	1356.229120	14.738752
20.382506	1359.993584	14.743770
20.425755	1361.833679	14.748787
20.107556	1342.782474	14.753805
19.849876	1339.433532	14.758823
20.289080	1347.167774	14.763840
20.467350	1353.172432	14.768858
19.964026	1350.739345	14.773875
20.448025	1351.791505	14.778893
20.420611	1354.254706	14.783911
20.233472	1359.708077	14.788928
20.256785	1351.281204	14.793946
20.306114	1363.668509	14.798963
20.269325	1360.258968	14.803981
20.411573	1355.191466	14.808999
20.191090	1364.958544	14.814016
20.553484	1357.134953	14.819034
20.288467	1368.089305	14.824051
20.196449	1364.225926	14.829069
20.525164	1363.453051	14.834087
20.318619	1366.123866	14.839104
20.027091	1358.925875	14.844122
20.211930	1367.087281	14.849139
20.013326	1366.648574	14.854157
20.206748	1358.618322	14.859175
20.325010	1382.563688	14.864192
20.383452	1386.241787	14.869210
20.514547	1392.018056	14.874227
20.968924	1398.755341	14.879245
20.727082	1396.585634	14.884263
20.258190	1392.653163	14.889280
20.800925	1393.944808	14.894298
20.740286	1393.847026	14.899315
21.135506	1385.367603	14.904333
21.199783	1398.688664	14.909351
20.809336	1392.858589	14.914368
21.123627	1388.127934	14.919386
20.935999	1381.255241	14.924403
20.904971	1370.709836	14.929421
21.058182	1363.374811	14.934439
20.647351	1353.691115	14.939456
20.564208	1362.195709	14.944474
20.789241	1376.699556	14.949491
20.892784	1390.440870	14.954509
21.232245	1389.641411	14.959527
21.147023	1390.777994	14.964544
21.385241	1377.977800	14.969562
21.298303	1372.471482	14.974579
20.788984	1360.315556	14.979597
21.080560	1356.221337	14.984615
21.033847	1380.913297	14.989632
21.214478	1377.606329	14.994650
21.166088	1383.805222	14.999667
21.419700	1384.010907	15.004685
21.170312	1360.766470	15.009703
21.090816	1361.832812	15.014720
21.210652	1363.635028	15.019738
21.245293	1367.364308	15.024755
21.139182	1379.117535	15.029773
21.356759	1379.424460	15.034791
21.253661	1378.963638	15.039808
21.628024	1375.637187	15.044826
21.319216	1384.420890	15.049843
21.242135	1371.946925	15.054861
21.295678	1375.400641	15.059879
21.048811	1386.896479	15.064896
21.235471	1387.520724	15.069914
21.408925	1382.020494	15.074931
21.071210	1379.150142	15.079949
21.290024	1380.132835	15.084967
20.983895	1381.990631	15.089984
21.028274	1385.306499	15.095002
21.200826	1390.414496	15.100019
21.449068	1401.943709	15.105037
21.709921	1402.332444	15.110055
21.491617	1408.475234	15.115072
21.522542	1411.461451	15.120090
21.488848	1415.154028	15.125107
21.610922	1408.467040	15.130125
21.742039	1411.343754	15.135143
21.680512	1419.919602	15.140160
21.902857	1414.279377	15.145178
22.002934	1422.757207	15.150195
21.714757	1417.170026	15.155213
21.731461	1406.646613	15.160231
22.038573	1419.169617	15.165248
22.047998	1411.069810	15.170266
21.937222	1409.813027	15.175283
21.928731	1418.661583	15.180301
22.133257	1411.975507	15.185319
21.816962	1419.353013	15.190336
21.969938	1406.956275	15.195354
22.105325	1418.661274	15.200371
22.099481	1407.244758	15.205389
22.286177	1410.365020	15.210407
21.939310	1410.204795	15.215424
21.904640	1414.100679	15.220442
21.831115	1407.393722	15.225459
21.999376	1411.356393	15.230477
22.117963	1411.547036	15.235495
22.072624	1415.354532	15.240512
21.987002	1407.535816	15.245530
21.540061	1414.638108	15.250547
21.742041	1411.170119	15.255565
21.900407	1405.904265	15.260583
22.027981	1409.050852	15.265600
22.124012	1410.910165	15.270618
22.081707	1427.968525	15.275635
22.128293	1438.456372	15.280653
22.526041	1438.900390	15.285671
22.122589	1441.613667	15.290688
22.106411	1443.943527	15.295706
22.256759	1439.991963	15.300723
22.274696	1440.028804	15.305741
22.621159	1432.448756	15.310759
22.721171	1434.970394	15.315776
22.645680	1439.208472	15.320794
22.714755	1436.974674	15.325811
22.793048	1448.183644	15.330829
22.793780	1443.056872	15.335847
22.512225	1443.051578	15.340864
22.652128	1445.363465	15.345882
22.637621	1438.149877	15.350899
22.778528	1442.767470	15.355917
22.903864	1436.556696	15.360935
22.419317	1438.807031	15.365952
22.651751	1436.046582	15.370970
22.798938	1426.686964	15.375987
22.596830	1433.146761	15.381005
22.773983	1422.362126	15.386023
22.616073	1435.791664	15.391040
22.666692	1439.851381	15.396058
22.878813	1430.901474	15.401075
22.545239	1434.181516	15.406093
23.136503	1425.377486	15.411111
22.773997	1437.755884	15.416128
22.814321	1435.105593	15.421146
23.444525	1430.722212	15.426163
23.006064	1437.715631	15.431181
22.875973	1434.171921	15.436199
22.679443	1436.005275	15.441216
22.767836	1436.691069	15.446234
22.739530	1425.525894	15.451251
22.752298	1442.000356	15.456269
22.723992	1431.155251	15.461287
22.654322	1443.463113	15.466304
23.034181	1458.584302	15.471322
23.120957	1459.171154	15.476339
22.996376	1463.850039	15.481357
23.593980	1458.508282	15.486375
23.352831	1464.204883	15.491392
23.273415	1466.740885	15.496410
23.633665	1464.725791	15.501427
23.252889	1471.321489	15.506445
23.524678	1461.838855	15.511463
23.495872	1455.892965	15.516480
23.154099	1452.792173	15.521498
23.654894	1457.410015	15.526515
23.449656	1453.314185	15.531533
23.583000	1448.994180	15.536551
23.319277	1439.815196	15.541568
23.087207	1437.493079	15.546586
23.789168	1454.734122	15.551603
23.620694	1464.091080	15.556621
23.485221	1456.271933	15.561639
23.587534	1456.582987	15.566656
23.650135	1451.729428	15.571674
23.829727	1456.373295	15.576691
23.757380	1445.650039	15.581709
23.499942	1435.233026	15.586727
23.561030	1436.497743	15.591744
23.270339	1441.728531	15.596762
23.365993	1453.402340	15.601779
23.597403	1454.108546	15.606797
23.747759	1453.332919	15.611815
23.456636	1454.117781	15.616832
23.467206	1446.196110	15.621850
23.589643	1447.883733	15.626867
23.143354	1460.684679	15.631885
23.493084	1475.245526	15.636903
24.026934	1485.554686	15.641920
23.908601	1482.997588	15.646938
24.230098	1472.137048	15.651955
24.173411	1486.127419	15.656973
24.071056	1481.032272	15.661991
24.249267	1480.758324	15.667008
23.688438	1487.036999	15.672026
24.294397	1476.370292	15.677043
23.877633	1480.763319	15.682061
23.917245	1476.641896	15.687079
24.223646	1473.677462	15.692096
24.205631	1485.162641	15.697114
24.579558	1479.318946	15.702131
24.183678	1490.631272	15.707149
24.193345	1473.879128	15.712167
24.692640	1476.313788	15.717184
24.159901	1480.185475	15.722202
24.158331	1470.898889	15.727219
24.010094	1480.507227	15.732237
24.216749	1474.421946	15.737255
24.122177	1465.503121	15.742272
24.262012	1467.920140	15.747290
24.558306	1473.577745	15.752307
24.267486	1481.550267	15.757325
23.981417	1483.280738	15.762343
24.090305	1475.221906	15.767360
24.372136	1498.967533	15.772378
24.850062	1494.261324	15.777395
24.588801	1499.515210	15.782413
24.835817	1501.436931	15.787431
24.634601	1494.112111	15.792448
24.486242	1489.880476	15.797466
24.964810	1481.971050	15.802483
24.550929	1485.181725	15.807501
24.901881	1485.785855	15.812519
24.685027	1481.439581	15.817536
24.848488	1491.723467	15.822554
24.881381	1490.452334	15.827571
24.627675	1479.479169	15.832589
24.855352	1493.491354	15.837607
24.884780	1495.877842	15.842624
24.863760	1496.939234	15.847642
25.317338	1491.200454	15.852659
24.955990	1486.520237	15.857677
24.763019	1472.120522	15.862695
25.145560	1476.811496	15.867712
24.987928	1474.837672	15.872730
24.955474	1466.451467	15.877747
24.603571	1472.320740	15.882765
24.970446	1493.097588	15.887783
25.083362	1491.685252	15.892800
25.020169	1499.597648	15.897818
25.120437	1495.677985	15.902835
25.220070	1494.952094	15.907853
24.702604	1500.858243	15.912871
25.020703	1496.422985	15.917888
25.232407	1499.264323	15.922906
25.170976	1490.484089	15.927923
25.065335	1498.972012	15.932941
25.200727	1484.219882	15.937959
25.326847	1493.716655	15.942976
25.072446	1497.178873	15.947994
25.379265	1491.033692	15.953011
25.333485	1496.145990	15.958029
25.416948	1501.435704	15.963047
25.468396	1499.778826	15.968064
25.429511	1517.390255	15.973082
26.058596	1517.585340	15.978099
25.775765	1504.843767	15.983117
25.738638	1490.789484	15.988135
25.714211	1489.364460	15.993152
25.799210	1489.776413	15.998170
25.891263	1485.237647	16.003187
25.780821	1490.162621	16.008205
25.409811	1493.746116	16.013223
25.913863	1481.648265	16.018240
25.578822	1500.209494	16.023258
25.663118	1488.302013	16.028275
25.907074	1489.444327	16.033293
25.684982	1489.845323	16.038311
25.708047	1480.520399	16.043328
25.641154	1494.674671	16.048346
25.721319	1479.784055	16.053363
25.760977	1503.321763	16.058381
26.007895	1510.493449	16.063399
26.145983	1513.966266	16.068416
25.890513	1519.685337	16.073434
26.151709	1510.641038	16.078451
25.929944	1514.371081	16.083469
25.961144	1508.655389	16.088487
26.312942	1514.993969	16.093504
26.061530	1517.112008	16.098522
26.142859	1518.306058	16.103539
26.378591	1523.622533	16.108557
26.455921	1513.983488	16.113575
26.451450	1503.036749	16.118592
25.962213	1491.662030	16.123610
26.278684	1489.698277	16.128627
26.558388	1502.330217	16.133645
26.110813	1501.449667	16.138663
25.873162	1498.654454	16.143680
25.934963	1515.094496	16.148698
26.199130	1515.253554	16.153715
25.918946	1526.227851	16.158733
26.108025	1522.556858	16.163751
26.128788	1512.257503	16.168768
25.690831	1518.797336	16.173786
26.366826	1531.098324	16.178803
26.391260	1540.096220	16.183821
26.539773	1544.666128	16.188839
26.743509	1537.272654	16.193856
26.110412	1545.634562	16.198874
26.575274	1546.069833	16.203891
26.630177	1540.772642	16.208909
26.628856	1540.987080	16.213927
26.766014	1541.727796	16.218944
27.228152	1537.050173	16.223962
26.900221	1540.372609	16.228979
26.985733	1542.239978	16.233997
26.629521	1551.444220	16.239015
26.988466	1543.768745	16.244032
26.652178	1551.149229	16.249050
26.843407	1538.485031	16.254067
27.025867	1540.063514	16.259085
27.270143	1545.185669	16.264103
26.987857	1547.232842	16.269120
26.903628	1551.321217	16.274138
27.009778	1545.821052	16.279155
26.991161	1540.372257	16.284173
26.901463	1544.780432	16.289191
27.216340	1530.256015	16.294208
27.207071	1549.842482	16.299226
27.049908	1545.881578	16.304243
27.206249	1532.855841	16.309261
27.311920	1543.697358	16.314279
27.132938	1540.287703	16.319296
27.018751	1536.863775	16.324314
27.237474	1537.995704	16.329331
27.249387	1548.436218	16.334349
27.420968	1558.530617	16.339367
27.557055	1542.729899	16.344384
27.332821	1555.297301	16.349402
27.352514	1560.642084	16.354419
27.612137	1563.226682	16.359437
27.537011	1574.557999	16.364455
27.756777	1557.220584	16.369472
27.681161	1549.534390	16.374490
27.669418	1528.570804	16.379507
27.589567	1529.531705	16.384525
27.540833	1531.151621	16.389543
27.630880	1529.653700	16.394560
27.560202	1534.881943	16.399578
27.787225	1556.267463	16.404595
27.804273	1552.871799	16.409613
27.770289	1561.462849	16.414631
28.079876	1551.450677	16.419648
27.869325	1542.646288	16.424666
27.426979	1537.025932	16.429683
27.323269	1546.729299	16.434701
27.596629	1564.832773	16.439719
27.875120	1562.733568	16.444736
27.582300	1565.442325	16.449754
27.662544	1567.642064	16.454771
28.062243	1561.962181	16.459789
27.804432	1574.729253	16.464807
28.097648	1568.485901	16.469824
27.943270	1566.996956	16.474842
28.000854	1565.922909	16.479859
27.993345	1577.426889	16.484877
28.077017	1584.950836	16.489895
28.258137	1592.385817	16.494912
28.018439	1587.906682	16.499930
28.212815	1599.159531	16.504947
28.501441	1585.531139	16.509965
27.899256	1593.258428	16.514983
28.364630	1583.682247	16.520000
28.335177	1588.596597	16.525018
28.281188	1593.716586	16.530035
28.383173	1590.384801	16.535053
28.266219	1587.964070	16.540071
28.339203	1592.878781	16.545088
28.254072	1590.365774	16.550106
28.376300	1588.871573	16.555123
28.526033	1583.628743	16.560141
28.360380	1577.231060	16.565159
28.728475	1582.786659	16.570176
28.774563	1582.560573	16.575194
28.856289	1584.110072	16.580211
28.873554	1583.254117	16.585229
28.418558	1592.652693	16.590247
28.579898	1586.713454	16.595264
28.589652	1588.952822	16.600282
28.451718	1607.803191	16.605299
28.388107	1609.653924	16.610317
28.893128	1622.553374	16.615335
29.123075	1615.925994	16.620352
29.346657	1616.713032	16.625370
28.900016	1613.768547	16.630387
29.206964	1602.020171	16.635405
29.109909	1616.936633	16.640423
29.163121	1603.366106	16.645440
29.217983	1604.505097	16.650458
29.091604	1583.537978	16.655475
28.881437	1581.163394	16.660493
28.955881	1606.175411	16.665511
29.204788	1605.878731	16.670528
29.380639	1610.781925	16.675546
29.329814	1602.820734	16.680563
29.265321	1603.139729	16.685581
29.155430	1602.446167	16.690599
29.275624	1602.440091	16.695616
29.411146	1604.069266	16.700634
29.013129	1611.590709	16.705651
29.605977	1596.915083	16.710669
29.356340	1606.216669	16.715687
29.842789	1604.553493	16.720704
29.724373	1594.785789	16.725722
29.432998	1609.321825	16.730739
29.837167	1601.338440	16.735757
29.497941	1609.656049	16.740775
29.360513	1600.328890	16.745792
29.496242	1604.194243	16.750810
29.668223	1605.400847	16.755827
29.656609	1600.495358	16.760845
29.652371	1610.867329	16.765863
29.674394	1603.120452	16.770880
29.663481	1606.077414	16.775898
29.455055	1605.842687	16.780915
29.667153	1598.215124	16.785933
29.510530	1604.586752	16.790951
29.507841	1601.137653	16.795968
29.600627	1614.295518	16.800986
29.557406	1636.562117	16.806003
29.700211	1631.620023	16.811021
29.830799	1642.000003	16.816039
29.826070	1634.629587	16.821056
29.905192	1636.619680	16.826074
29.642452	1637.409692	16.831091
29.865258	1627.262236	16.836109
29.899157	1649.008997	16.841127
30.195180	1656.685611	16.846144
30.418390	1659.630585	16.851162
30.496394	1653.753940	16.856179
30.887837	1649.757675	16.861197
30.681633	1637.549760	16.866215
30.223083	1625.554113	16.871232
30.359217	1614.784405	16.876250
30.145604	1623.682006	16.881267
30.345931	1616.998900	16.886285
30.150154	1608.116831	16.891303
30.561588	1637.252214	16.896320
30.772026	1645.844568	16.901338
30.696074	1635.478863	16.906355
30.780520	1619.204336	16.911373
30.422437	1626.768386	16.916391
30.672517	1623.423488	16.921408
30.448597	1624.034630	16.926426
30.177745	1639.345641	16.931443
30.578244	1642.342356	16.936461
30.539237	1652.806333	16.941479
30.450692	1656.102539	16.946496
31.137506	1653.316022	16.951514
30.910189	1659.073395	16.956531
30.732348	1651.698172	16.961549
31.010414	1659.173824	16.966567
30.814175	1655.133536	16.971584
30.994588	1653.126939	16.976602
30.608602	1664.086176	16.981619
30.996238	1647.053933	16.986637
30.867072	1645.923798	16.991655
30.781259	1651.135295	16.996672
31.132429	1648.879950	17.001690
30.874499	1646.202241	17.006707
31.090492	1650.523604	17.011725
31.451708	1656.951235	17.016743
31.197439	1657.968192	17.021760
31.286406	1646.955485	17.026778
30.997664	1656.223812	17.031795
31.431937	1665.418481	17.036813
31.606872	1666.295467	17.041831
31.361566	1674.767243	17.046848
31.445685	1663.769106	17.051866
31.235976	1671.849553	17.056883
31.668664	1668.786611	17.061901
31.566401	1674.063045	17.066919
31.419943	1672.360180	17.071936
31.531466	1669.558688	17.076954
31.496616	1675.956244	17.081971
31.795407	1667.331220	17.086989
31.826883	1668.528812	17.092007
31.824347	1671.222195	17.097024
32.140788	1662.308818	17.102042
31.890562	1657.838099	17.107059
31.670733	1645.236371	17.112077
31.586169	1655.566949	17.117095
31.720395	1665.536501	17.122112
31.937256	1659.938828	17.127130
31.803621	1670.359038	17.132147
32.059317	1662.332885	17.137165
31.973139	1674.152326	17.142183
31.516500	1672.960274	17.147200
31.975431	1662.326056	17.152218
31.836257	1673.808602	17.157235
31.717610	1667.893650	17.162253
32.118206	1668.199803	17.167271
31.953387	1677.424788	17.172288
31.989108	1661.353561	17.177306
31.971831	1676.820649	17.182323
32.459450	1683.913974	17.187341
32.328508	1690.254219	17.192359
32.539482	1694.532332	17.197376
32.670314	1674.587461	17.202394
32.118430	1673.646614	17.207411
32.523648	1665.993731	17.212429
32.534917	1659.244670	17.217447
32.436080	1658.054787	17.222464
32.563716	1662.073856	17.227482
32.497675	1666.648226	17.232499
32.357153	1668.699104	17.237517
32.764565	1676.528543	17.242535
32.148665	1689.077446	17.247552
32.693940	1688.173026	17.252570
32.467802	1688.635325	17.257587
32.308563	1696.099158	17.262605
32.612845	1689.673217	17.267623
32.850105	1699.065098	17.272640
32.727084	1688.621718	17.277658
32.653360	1690.812718	17.282675
32.658778	1694.204396	17.287693
32.717766	1697.699408	17.292711
32.394442	1696.574648	17.297728
32.589933	1701.684462	17.302746
32.769674	1719.821730	17.307763
33.360850	1723.952246	17.312781
33.505714	1721.312548	17.317799
33.274816	1720.698467	17.322816
33.662789	1712.727157	17.327834
33.565351	1701.128741	17.332851
33.215820	1688.396093	17.337869
33.354151	1691.193319	17.342887
33.450301	1691.289257	17.347904
33.492831	1686.892491	17.352922
33.555643	1685.869539	17.357939
33.224866	1677.868841	17.362957
33.341599	1682.792478	17.367975
33.139582	1682.084640	17.372992
33.216154	1674.872789	17.378010
33.329538	1686.146200	17.383027
33.216349	1702.238645	17.388045
33.787812	1698.949174	17.393063
33.535497	1714.850497	17.398080
34.182581	1706.624077	17.403098
33.651807	1711.297858	17.408115
33.567391	1715.028826	17.413133
33.653569	1714.935470	17.418151
33.515372	1713.142649	17.423168
33.823342	1703.683012	17.428186
33.773615	1708.717293	17.433203
33.677919	1707.546570	17.438221
33.819359	1704.358228	17.443239
33.285625	1704.595085	17.448256
33.733882	1704.085471	17.453274
33.362702	1712.043464	17.458291
33.735976	1730.166413	17.463309
34.086565	1734.537166	17.468327
34.164462	1741.254663	17.473344
33.937698	1745.850159	17.478362
33.814001	1745.673052	17.483379
33.892524	1736.779739	17.488397
34.248435	1740.099607	17.493415
34.259797	1740.221003	17.498432
34.134615	1742.611872	17.503450
34.129866	1736.228424	17.508467
34.044281	1743.960793	17.513485
34.538206	1745.651894	17.518503
34.303970	1748.818700	17.523520
34.631894	1760.121206	17.528538
34.735410	1757.026141	17.533555
34.545668	1749.189848	17.538573
34.972196	1743.043644	17.543591
34.708540	1737.878271	17.548608
34.803245	1739.527606	17.553626
34.668905	1734.439247	17.558643
34.604304	1736.511813	17.563661
34.640550	1733.988919	17.568679
34.428429	1743.169413	17.573696
34.873072	1744.951747	17.578714
34.766919	1741.776837	17.583731
34.554309	1754.246018	17.588749
34.609664	1749.224668	17.593767
34.910485	1764.941138	17.598784
34.595284	1766.163862	17.603802
34.693615	1763.912180	17.608819
35.001989	1769.142695	17.613837
35.207816	1763.058227	17.618855
34.954522	1764.502590	17.623872
35.203536	1760.232637	17.628890
35.092214	1762.976727	17.633907
35.094318	1762.783119	17.638925
35.362284	1759.758067	17.643943
35.317034	1764.062486	17.648960
35.403523	1756.807616	17.653978
35.543333	1763.102269	17.658995
35.291464	1751.869942	17.664013
35.440592	1759.344159	17.669031
35.399568	1761.071878	17.674048
35.427886	1752.393957	17.679066
35.664478	1755.471774	17.684083
35.543586	1750.723704	17.689101
35.519790	1752.482821	17.694119
35.746267	1754.632781	17.699136
35.786869	1749.972536	17.704154
35.653141	1751.924268	17.709171
35.603203	1755.046383	17.714189
35.876293	1754.138606	17.719207
35.600344	1755.803651	17.724224
35.913086	1765.573233	17.729242
36.299494	1773.686122	17.734259
35.385852	1761.495255	17.739277
35.938698	1770.171137	17.744295
35.823506	1782.921849	17.749312
35.741617	1778.040933	17.754330
35.790065	1776.471923	17.759347
36.051105	1785.854801	17.764365
35.943434	1768.085935	17.769383
36.193332	1784.470312	17.774400
36.332234	1784.811929	17.779418
36.150172	1778.403888	17.784435
35.836862	1787.594865	17.789453
36.493088	1787.203174	17.794471
35.968406	1771.800227	17.799488
36.138637	1777.898115	17.804506
36.183886	1799.343205	17.809523
36.354577	1801.558709	17.814541
36.533890	1804.415704	17.819559
36.581855	1809.315336	17.824576
36.597525	1813.109282	17.829594
36.995220	1803.166218	17.834611
36.382232	1824.986093	17.839629
36.339932	1813.028854	17.844647
36.437236	1807.235964	17.849664
36.315359	1807.803050	17.854682
36.657870	1814.222820	17.859699
36.813693	1808.687564	17.864717
36.771567	1805.709128	17.869735
36.498021	1808.511980	17.874752
36.799274	1799.677024	17.879770
36.988455	1814.354149	17.884787
36.855570	1836.701238	17.889805
37.105492	1833.927194	17.894823
37.151684	1834.184163	17.899840
37.192128	1836.456280	17.904858
37.419774	1829.826040	17.909875
36.763818	1822.724399	17.914893
37.154328	1822.712144	17.919911
37.382900	1837.627653	17.924928
37.076494	1835.078805	17.929946
37.450181	1827.729493	17.934963
37.230061	1836.275927	17.939981
37.290248	1831.582493	17.944999
37.394946	1834.347912	17.950016
37.366028	1833.348407	17.955034
37.729011	1826.282368	17.960051
37.909317	1831.141981	17.965069
37.519137	1831.540897	17.970087
37.111444	1833.613990	17.975104
37.397993	1832.079170	17.980122
37.819170	1833.731147	17.985139
37.577783	1835.932609	17.990157
37.611469	1827.727778	17.995175
37.421696	1834.277432	18.000192
37.445576	1833.599109	18.005210
37.704806	1829.792017	18.010227
37.655832	1838.782164	18.015245
37.775933	1844.982868	18.020263
37.778462	1854.343633	18.025280
38.068787	1861.112227	18.030298
38.229030	1852.387995	18.035315
37.854158	1859.232093	18.040333
37.802021	1859.947870	18.045351
37.830660	1857.158102	18.050368
38.121135	1864.338095	18.055386
38.098700	1852.878722	18.060403
38.164717	1865.487289	18.065421
38.080255	1850.161762	18.070439
38.157238	1845.198611	18.075456
38.147863	1865.583928	18.080474
38.785073	1867.883609	18.085491
38.558056	1872.215401	18.090509
38.702655	1871.895438	18.095527
38.921907	1853.127444	18.100544
38.341711	1841.187207	18.105562
38.507393	1842.707869	18.110579
38.448498	1855.256008	18.115597
38.800741	1855.861122	18.120615
38.632511	1870.562445	18.125632
38.861505	1879.423907	18.130650
39.276480	1879.642251	18.135667
39.051099	1867.470007	18.140685
38.845109	1856.833951	18.145703
38.927319	1853.195539	18.150720
38.537612	1858.290891	18.155738
38.867538	1865.937192	18.160755
38.799909	1883.431747	18.165773
38.672636	1871.138135	18.170791
39.051680	1875.119566	18.175808
38.951497	1879.467760	18.180826
39.346651	1873.383787	18.185843
39.226401	1879.770371	18.190861
39.125963	1867.932167	18.195879
39.214842	1868.530891	18.200896
39.054606	1870.483877	18.205914
39.167711	1867.843115	18.210931
38.574501	1883.906967	18.215949
39.407876	1891.139593	18.220967
39.716422	1898.352830	18.225984
39.583767	1907.916724	18.231002
40.039143	1895.689605	18.236019
39.915526	1896.022727	18.241037
39.586170	1896.047786	18.246055
40.347277	1894.857219	18.251072
39.820638	1888.136894	18.256090
39.907307	1862.762009	18.261107
40.065761	1864.720097	18.266125
39.622205	1859.607308	18.271143
39.545018	1860.667002	18.276160
39.297941	1869.256107	18.281178
39.849166	1878.813826	18.286195
39.640898	1893.621409	18.291213
39.802986	1888.477613	18.296231
39.960223	1890.684727	18.301248
39.607733	1900.900384	18.306266
40.121618	1889.266740	18.311283
39.685901	1895.863051	18.316301
39.868591	1902.214047	18.321319
40.613960	1921.364992	18.326336
40.379238	1923.023226	18.331354
40.091829	1923.555915	18.336371
40.219931	1930.067145	18.341389
40.031466	1924.430589	18.346407
40.276134	1920.063279	18.351424
40.025970	1934.601849	18.356442
40.718482	1930.889917	18.361459
40.275155	1925.747934	18.366477
40.467180	1928.793008	18.371495
40.707725	1932.904083	18.376512
40.262511	1948.151748	18.381530
40.714335	1948.001780	18.386547
40.691615	1948.128427	18.391565
40.621814	1946.602999	18.396583
41.043773	1938.158221	18.401600
40.739696	1948.007223	18.406618
40.786083	1944.782603	18.411635
40.861542	1940.856700	18.416653
40.681607	1938.230198	18.421671
40.908536	1931.419323	18.426688
40.893112	1951.408897	18.431706
41.159920	1937.402307	18.436723
40.928327	1946.750715	18.441741
41.097813	1959.085526	18.446759
41.549175	1963.145164	18.451776
41.474448	1973.544404	18.456794
41.432072	1969.030121	18.461811
41.393941	1967.327395	18.466829
41.404817	1964.042508	18.471847
41.974966	1957.369279	18.476864
41.498531	1959.674641	18.481882
41.795427	1952.673821	18.486899
41.829155	1955.243135	18.491917
41.547121	1938.065163	18.496935
41.896553	1945.170075	18.501952
41.735521	1942.267603	18.506970
41.359584	1933.183679	18.511987
42.036574	1954.910207	18.517005
42.209205	1962.164091	18.522023
42.001468	1945.245073	18.527040
41.772774	1945.735755	18.532058
41.937930	1954.433813	18.537075
42.147145	1962.990719	18.542093
41.510899	1961.055928	18.547111
42.320291	1956.202173	18.552128
41.814494	1963.153825	18.557146
41.950149	1953.759973	18.562163
42.170413	1946.531683	18.567181
41.801754	1959.567035	18.572199
42.091599	1956.555252	18.577216
42.444273	1951.418853	18.582234
42.080598	1960.725754	18.587251
42.719789	1950.483547	18.592269
42.314310	1954.602390	18.597287
42.342811	1951.385454	18.602304
42.537821	1975.090676	18.607322
42.445128	1977.968730	18.612339
42.416549	1982.511399	18.617357
42.558869	1987.562001	18.622375
42.764405	1980.977092	18.627392
42.527928	1986.884530	18.632410
42.509193	1980.972992	18.637427
42.668209	1985.588931	18.642445
42.602581	1979.013885	18.647463
42.885481	1977.283195	18.652480
43.055163	1978.487454	18.657498
42.683702	1972.178807	18.662515
43.118358	1980.840521	18.667533
42.807899	1985.054269	18.672551
43.305077	1978.986827	18.677568
43.205683	1992.972915	18.682586
43.147112	1991.642083	18.687603
43.347770	1989.579728	18.692621
43.503627	1998.982909	18.697639
43.606452	1997.579680	18.702656
43.287286	1978.011698	18.707674
43.391523	1979.567746	18.712691
43.746871	1991.739127	18.717709
43.202864	1986.138194	18.722727
43.563629	1985.639124	18.727744
43.422355	2003.795630	18.732762
43.578888	2007.392672	18.737779
43.924118	2007.483589	18.742797
43.644076	2003.537796	18.747815
43.727623	2005.845321	18.752832
43.748683	1996.692864	18.757850
44.176917	1999.788211	18.762867
44.080085	1986.943785	18.767885
43.780938	2009.713150	18.772903
43.980227	1993.790482	18.777920
43.804884	1995.994810	18.782938
43.786961	2001.283767	18.787955
43.783744	2002.778081	18.792973
43.695043	2012.993044	18.797991
43.843155	2004.489244	18.803008
44.500367	2017.313037	18.808026
44.259338	2025.970519	18.813043
43.966589	2023.746157	18.818061
43.913394	2030.842581	18.823079
44.294476	2017.092594	18.828096
44.260571	2036.078622	18.833114
44.197019	2022.532970	18.838131
44.523263	2031.630784	18.843149
44.357919	2027.289605	18.848167
44.562466	2048.979928	18.853184
44.725217	2058.776108	18.858202
44.863413	2057.009921	18.863219
45.184832	2055.253159	18.868237
45.127685	2048.255803	18.873255
45.320897	2033.893194	18.878272
45.310173	2017.755666	18.883290
45.248983	2007.642391	18.888307
45.380289	2010.579424	18.893325
45.547535	2007.509191	18.898343
45.702231	2004.331585	18.903360
45.468687	2008.977101	18.908378
45.435891	2013.214565	18.913395
45.403659	1985.998102	18.918413
45.131126	1985.014124	18.923431
45.276092	1981.597185	18.928448
45.239533	1991.537352	18.933466
45.324729	2007.921285	18.938483
45.404296	2008.291631	18.943501
45.320825	2018.230529	18.948519
45.294936	2007.859434	18.953536
45.423149	2013.251365	18.958554
44.976079	2018.224374	18.963571
45.003156	2009.834710	18.968589
45.014891	2023.415801	18.973607
45.323571	2028.530998	18.978624
45.249167	2033.337181	18.983642
45.333063	2044.361399	18.988659
45.587554	2045.840603	18.993677
45.353608	2051.412599	18.998695
45.655491	2059.495147	19.003712
46.050132	2062.818516	19.008730
45.945010	2060.301655	19.013747
46.151419	2061.643150	19.018765
46.120555	2060.721120	19.023783
46.139416	2070.199393	19.028800
46.307902	2064.295405	19.033818
46.332766	2062.129076	19.038835
46.489964	2055.479303	19.043853
46.558924	2063.954369	19.048871
46.565764	2062.002842	19.053888
46.562832	2063.383332	19.058906
46.385470	2062.587139	19.063923
46.339655	2064.557423	19.068941
46.350324	2055.210978	19.073959
46.598859	2055.517518	19.078976
46.555826	2059.327939	19.083994
46.648587	2078.595019	19.089011
46.953634	2079.337096	19.094029
46.904454	2097.880047	19.099047
47.044217	2091.192200	19.104064
46.909841	2092.837380	19.109082
46.923463	2093.998197	19.114099
47.123785	2085.758550	19.119117
46.938750	2088.936568	19.124135
46.977890	2081.713404	19.129152
47.069396	2084.714524	19.134170
47.113502	2084.310801	19.139187
47.043774	2087.768553	19.144205
46.922334	2094.357002	19.149223
47.141795	2085.804728	19.154240
47.157684	2082.893405	19.159258
47.169829	2105.734595	19.164275
47.471570	2099.693564	19.169293
47.356057	2116.107304	19.174311
47.446747	2114.287952	19.179328
47.579631	2104.636980	19.184346
47.384484	2105.923709	19.189363
47.600552	2105.701753	19.194381
47.457941	2110.899187	19.199399
47.566951	2102.996314	19.204416
47.803892	2110.353007	19.209434
47.824294	2132.797189	19.214451
48.012998	2135.786554	19.219469
48.127538	2135.125490	19.224487
47.892129	2130.797459	19.229504
48.551892	2130.855979	19.234522
48.239858	2132.021117	19.239539
48.406597	2127.812721	19.244557
48.540208	2136.504687	19.249575
48.489179	2126.612100	19.254592
48.582618	2125.409239	19.259610
48.408263	2116.866253	19.264627
48.595875	2099.837898	19.269645
48.581437	2101.758502	19.274663
48.293507	2095.090293	19.279680
48.574151	2108.586771	19.284698
48.964654	2117.233432	19.289715
48.744582	2108.789756	19.294733
48.692146	2104.215679	19.299751
48.509619	2113.472595	19.304768
48.420882	2117.365403	19.309786
48.710605	2125.073610	19.314803
48.873695	2125.437609	19.319821
48.902599	2133.087825	19.324839
48.881588	2131.580284	19.329856
48.983160	2127.616938	19.334874
49.136479	2126.212030	19.339891
49.072057	2124.179378	19.344909
48.832659	2121.749704	19.349927
48.897934	2124.972504	19.354944
49.018759	2138.374997	19.359962
48.984348	2160.677110	19.364979
48.937591	2160.566393	19.369997
49.378063	2159.165509	19.375015
49.281063	2162.188409	19.380032
49.570472	2158.582546	19.385050
49.350123	2164.583841	19.390067
49.223297	2156.060523	19.395085
49.174877	2170.263927	19.400103
49.254534	2182.931912	19.405120
49.627373	2192.527241	19.410138
49.724811	2197.697946	19.415155
49.967212	2189.455214	19.420173
49.865989	2187.721177	19.425191
49.945857	2183.813382	19.430208
50.424669	2182.336459	19.435226
50.089208	2183.612964	19.440243
50.333809	2178.732190	19.445261
50.273441	2176.294123	19.450279
50.154871	2180.443470	19.455296
50.317187	2178.794933	19.460314
50.192919	2177.232829	19.465331
50.341688	2175.709375	19.470349
50.305093	2184.745705	19.475367
50.095175	2195.339926	19.480384
50.484626	2205.905380	19.485402
50.593193	2204.095657	19.490419
50.617454	2211.767941	19.495437
50.895424	2198.722295	19.500455
50.650439	2202.840610	19.505472
51.157463	2199.422334	19.510490
50.874979	2214.138963	19.515507
51.067299	2213.567776	19.520525
51.026079	2204.748356	19.525543
50.910662	2206.031734	19.530560
51.146344	2204.466325	19.535578
50.986751	2203.514814	19.540595
51.041444	2204.601907	19.545613
51.157806	2199.907722	19.550631
50.839913	2207.393739	19.555648
51.257743	2195.681283	19.560666
50.904608	2204.609798	19.565683
51.476179	2208.579910	19.570701
51.679462	2228.372988	19.575719
51.495350	2234.927778	19.580736
51.364951	2234.365540	19.585754
51.406023	2238.560517	19.590771
51.946479	2228.158883	19.595789
52.035976	2232.614353	19.600807
51.577160	2232.406902	19.605824
51.939562	2219.572463	19.610842
51.778963	2237.356837	19.615859
51.712217	2229.918452	19.620877
51.987633	2220.745399	19.625895
51.951461	2224.359048	19.630912
52.143462	2223.635152	19.635930
52.079445	2222.263862	19.640947
52.110241	2228.003113	19.645965
52.130723	2228.333246	19.650983
51.853684	2227.147235	19.656000
52.152914	2217.911971	19.661018
52.249971	2217.286477	19.666035
52.141660	2225.970520	19.671053
52.198920	2225.401618	19.676071
51.931543	2241.132343	19.681088
52.216545	2242.615964	19.686106
52.496588	2253.527926	19.691123
52.363925	2250.977404	19.696141
52.385516	2243.569269	19.701159
52.744142	2252.079152	19.706176
52.504085	2245.859267	19.711194
52.622276	2267.719320	19.716211
52.679308	2273.232581	19.721229
52.914835	2281.149848	19.726247
52.972954	2286.928693	19.731264
53.030640	2278.063718	19.736282
53.017384	2277.874616	19.741299
53.182751	2282.763618	19.746317
53.196696	2281.204997	19.751335
53.045883	2287.027887	19.756352
53.408468	2268.503781	19.761370
53.479730	2276.681720	19.766387
53.098095	2274.596453	19.771405
53.461608	2273.791003	19.776423
53.617868	2285.784551	19.781440
53.910647	2288.239762	19.786458
53.547609	2300.050402	19.791475
53.758779	2297.699641	19.796493
54.255752	2291.354544	19.801511
53.760445	2289.688901	19.806528
53.873758	2286.747234	19.811546
54.223542	2289.534359	19.816563
54.030955	2287.885915	19.821581
54.169591	2287.696465	19.826599
54.188522	2289.738736	19.831616
54.492566	2287.240309	19.836634
54.242788	2290.325935	19.841651
54.354521	2280.854741	19.846669
54.518687	2283.421410	19.851687
54.314711	2289.468468	19.856704
54.311059	2286.838700	19.861722
54.342581	2279.048573	19.866739
53.964312	2286.841488	19.871757
54.360080	2284.023530	19.876775
54.355440	2287.035491	19.881792
54.516081	2282.512696	19.886810
54.403791	2289.254049	19.891827
54.430880	2308.580323	19.896845
54.589825	2313.001875	19.901863
54.563668	2319.928199	19.906880
54.790337	2312.582139	19.911898
54.800739	2310.335490	19.916915
54.796962	2312.676813	19.921933
54.787392	2316.145520	19.926951
54.928327	2330.642532	19.931968
55.013734	2333.009643	19.936986
55.336796	2340.905753	19.942003
55.061292	2341.529794	19.947021
55.513303	2337.331981	19.952039
55.535980	2345.493985	19.957056
55.121234	2337.786781	19.962074
55.328668	2333.766481	19.967091
55.267214	2328.190640	19.972109
55.490478	2337.162767	19.977127
55.432770	2356.191711	19.982144
55.551768	2369.821488	19.987162
55.879872	2370.396762	19.992179
55.723827	2377.769048	19.997197
56.101321	2372.363824	20.002215
55.783970	2368.814290	20.007232
56.086561	2375.216496	20.012250
55.898683	2362.925049	20.017267
55.983082	2366.181741	20.022285
56.509339	2362.015724	20.027303
56.198139	2366.995479	20.032320
56.611332	2361.373314	20.037338
56.666114	2355.634114	20.042355
56.505493	2353.364201	20.047373
56.443416	2345.861992	20.052391
56.732220	2355.940650	20.057408
56.714084	2356.770510	20.062426
56.804772	2357.511875	20.067443
56.512984	2363.998718	20.072461
56.618453	2357.007761	20.077479
56.508283	2361.491606	20.082496
56.581626	2356.955686	20.087514
56.848050	2368.750733	20.092531
56.656700	2386.581709	20.097549
56.864496	2379.465919	20.102567
56.762940	2382.373469	20.107584
56.886716	2384.938181	20.112602
57.178160	2382.093777	20.117619
56.833977	2381.901988	20.122637
56.933523	2394.403852	20.127655
57.232004	2405.442403	20.132672
57.462756	2427.615946	20.137690
57.545744	2412.612548	20.142707
57.622115	2411.777076	20.147725
58.268160	2411.640618	20.152743
57.818487	2414.130204	20.157760
57.929541	2414.297700	20.162778
58.155150	2415.895902	20.167795
58.260611	2410.831000	20.172813
58.172806	2408.839980	20.177831
57.864483	2406.269698	20.182848
57.843591	2404.898337	20.187866
58.123723	2411.864146	20.192883
58.010024	2412.767316	20.197901
58.599046	2402.447688	20.202919
58.141048	2402.248365	20.207936
58.322130	2402.779085	20.212954
58.501838	2408.259875	20.217971
58.297217	2413.044035	20.222989
58.264613	2407.742928	20.228007
57.872142	2419.191191	20.233024
58.015794	2411.406448	20.238042
58.342470	2424.353821	20.243059
58.369787	2435.048298	20.248077
58.743208	2433.273042	20.253095
58.270516	2428.242449	20.258112
58.751606	2438.970063	20.263130
58.803959	2429.580663	20.268147
58.682368	2450.410939	20.273165
59.051315	2452.546857	20.278183
59.120832	2459.866476	20.283200
59.179413	2464.631085	20.288218
59.216922	2461.476730	20.293235
59.306998	2472.391955	20.298253
59.833991	2462.982604	20.303271
59.801633	2457.627107	20.308288
59.477671	2469.821975	20.313306
59.811595	2453.302499	20.318323
59.764348	2457.437353	20.323341
59.967959	2446.786612	20.328359
59.646365	2429.892612	20.333376
59.528629	2428.623904	20.338394
59.884374	2437.695418	20.343411
59.925020	2450.827191	20.348429
59.949492	2451.169268	20.353447
59.559178	2447.866849	20.358464
59.719542	2455.884452	20.363482
60.206457	2453.967165	20.368499
59.870660	2452.534553	20.373517
60.061593	2451.849409	20.378535
60.000923	2446.356470	20.383552
60.003262	2448.357413	20.388570
60.231912	2462.884515	20.393587
60.123834	2478.221365	20.398605
60.350354	2478.444549	20.403623
60.568909	2476.072458	20.408640
60.025198	2474.402210	20.413658
60.217626	2473.045129	20.418675
60.201519	2491.518896	20.423693
60.319914	2498.417426	20.428711
60.683833	2500.844750	20.433728
60.499174	2508.532482	20.438746
61.019347	2504.680445	20.443763
60.932898	2524.539988	20.448781
61.108252	2522.915243	20.453799
61.289807	2522.096996	20.458816
61.364567	2525.617931	20.463834
61.676168	2518.384097	20.468851
61.888536	2522.838991	20.473869
61.875604	2515.462429	20.478887
62.027181	2495.994987	20.483904
61.438090	2495.814613	20.488922
61.862903	2485.037844	20.493939
61.829282	2488.926736	20.498957
61.415355	2480.273211	20.503975
61.380274	2492.749808	20.508992
61.341092	2504.745571	20.514010
61.899410	2511.318492	20.519027
61.852564	2518.670006	20.524045
61.971197	2521.065111	20.529063
61.836275	2517.144370	20.534080
61.599894	2525.096989	20.539098
62.433295	2532.783882	20.544115
62.159462	2546.796989	20.549133
62.309045	2542.781885	20.554151
62.641856	2546.766424	20.559168
62.434807	2554.584272	20.564186
62.368185	2545.359393	20.569203
62.267893	2546.345788	20.574221
62.568362	2543.229768	20.579239
62.639263	2543.353517	20.584256
62.684715	2548.248679	20.589274
62.818555	2547.686378	20.594291
62.979933	2547.158101	20.599309
63.041518	2548.329515	20.604327
62.936420	2559.785023	20.609344
62.839392	2563.795857	20.614362
63.341916	2569.163010	20.619379
63.382492	2571.563961	20.624397
63.346105	2564.023927	20.629415
63.160555	2567.955713	20.634432
63.262855	2574.060046	20.639450
63.515460	2570.468846	20.644467
63.685768	2567.568480	20.649485
63.477950	2575.912874	20.654503
63.719958	2562.557507	20.659520
63.677187	2572.022668	20.664538
63.825149	2560.582987	20.669555
63.488443	2564.979591	20.674573
63.534323	2563.807408	20.679591
63.740168	2567.629895	20.684608
63.409220	2587.528429	20.689626
64.212548	2580.547415	20.694643
64.194300	2593.338645	20.699661
64.048697	2602.410985	20.704679
64.366054	2584.867280	20.709696
64.424234	2599.167604	20.714714
64.600371	2594.451198	20.719731
64.499400	2595.826315	20.724749
64.561311	2593.954583	20.729767
64.834189	2597.902993	20.734784
64.561997	2588.704254	20.739802
64.803136	2586.868203	20.744819
64.616060	2590.240372	20.749837
64.734463	2584.061000	20.754855
64.658279	2588.684174	20.759872
64.779505	2602.773262	20.764890
65.061390	2605.507905	20.769907
64.927366	2620.304276	20.774925
64.700920	2617.979865	20.779943
65.506250	2609.248793	20.784960
65.271040	2619.883712	20.789978
65.346114	2610.499496	20.794995
65.142883	2610.615879	20.800013
65.211121	2621.152125	20.805031
65.551127	2631.139014	20.810048
65.584329	2646.306957	20.815066
65.919794	2638.947454	20.820083
65.960516	2640.173121	20.825101
65.936941	2643.502872	20.830119
65.855714	2639.508639	20.835136
65.998698	2641.989893	20.840154
66.171556	2629.492823	20.845171
66.151772	2639.511340	20.850189
66.058578	2641.853738	20.855207
66.028526	2638.739669	20.860224
65.972640	2643.846929	20.865242
66.306478	2629.072275	20.870259
66.453463	2633.143515	20.875277
66.575494	2648.883402	20.880295
66.775613	2648.955832	20.885312
66.516541	2655.575576	20.890330
67.188826	2650.798652	20.895347
66.901883	2644.818274	20.900365
66.584514	2650.828338	20.905383
66.583989	2648.561794	20.910400
66.440960	2659.787421	20.915418
66.489091	2643.728480	20.920435
66.980526	2646.469379	20.925453
66.838912	2654.913096	20.930471
66.638747	2674.926316	20.935488
67.155418	2675.133349	20.940506
67.250713	2676.554720	20.945523
67.178301	2675.460388	20.950541
67.073311	2682.285352	20.955559
67.562095	2674.700432	20.960576
67.669276	2698.277985	20.965594
67.832443	2698.235266	20.970611
67.876553	2704.528037	20.975629
67.829611	2712.339926	20.980647
67.933858	2696.054696	20.985664
68.032251	2700.112739	20.990682
68.330937	2709.595857	20.995699
68.266093	2702.773508	21.000717
67.846496	2702.367413	21.005735
68.491335	2691.685967	21.010752
68.545734	2698.646762	21.015770
68.533421	2704.996123	21.020787
68.394337	2691.752178	21.025805
68.383434	2695.008972	21.030823
68.863362	2690.009147	21.035840
68.382849	2693.278342	21.040858
68.592040	2695.547448	21.045875
68.448725	2687.120275	21.050893
68.469069	2696.906973	21.055911
68.654653	2687.444959	21.060928
68.624837	2694.174404	21.065946
68.500245	2701.051838	21.070963
68.602481	2719.053099	21.075981
68.705749	2729.115081	21.080999
69.067323	2724.923480	21.086016
69.027834	2733.237723	21.091034
69.477446	2740.382718	21.096051
69.440348	2739.974314	21.101069
69.370467	2757.997820	21.106087
69.721851	2749.162692	21.111104
69.596502	2743.797295	21.116122
69.671046	2749.245616	21.121139
69.777556	2745.471861	21.126157
69.658283	2749.071043	21.131175
69.870080	2740.698433	21.136192
69.857412	2747.586885	21.141210
69.688948	2745.383177	21.146227
70.040652	2759.656700	21.151245
69.919680	2783.362718	21.156263
70.108141	2774.644324	21.161280
69.981876	2782.142587	21.166298
70.328764	2775.978853	21.171315
69.983145	2777.602778	21.176333
70.371312	2790.185132	21.181351
70.605333	2797.552874	21.186368
70.644301	2809.725314	21.191386
70.287263	2804.101782	21.196403
70.919405	2814.904654	21.201421
70.885608	2809.812678	21.206439
71.011581	2804.283195	21.211456
71.204718	2802.509403	21.216474
71.216032	2802.707199	21.221491
71.163463	2795.454005	21.226509
71.308966	2792.851427	21.231527
71.443321	2791.201158	21.236544
71.361917	2800.858300	21.241562
71.543854	2818.286989	21.246579
72.028519	2820.149842	21.251597
72.000190	2809.323465	21.256615
71.667037	2791.096635	21.261632
71.453854	2794.166456	21.266650
71.917280	2811.631997	21.271667
71.679455	2813.143975	21.276685
71.714178	2812.940622	21.281703
72.256961	2811.225871	21.286720
72.105781	2806.421857	21.291738
71.864817	2813.009138	21.296755
72.218883	2815.420820	21.301773
72.322665	2816.738035	21.306791
72.352012	2809.378350	21.311808
72.210512	2817.323280	21.316826
72.199559	2826.712062	21.321843
72.577234	2830.333707	21.326861
72.494867	2838.900794	21.331879
72.954128	2834.946945	21.336896
73.027001	2838.147767	21.341914
72.708422	2841.192526	21.346931
73.297638	2833.843281	21.351949
72.902843	2840.151692	21.356967
72.918473	2833.491170	21.361984
73.019213	2832.085851	21.367002
72.910028	2829.004140	21.372019
73.247297	2826.265464	21.377037
73.349880	2834.821217	21.382055
73.265003	2852.927637	21.387072
73.480146	2855.750547	21.392090
73.352498	2863.110092	21.397107
73.760496	2858.408367	21.402125
73.380255	2856.690533	21.407143
73.635170	2867.156267	21.412160
73.731744	2852.299420	21.417178
73.552412	2877.395665	21.422195
74.088686	2874.075955	21.427213
74.048887	2887.002107	21.432231
74.040187	2884.370712	21.437248
74.442300	2888.269056	21.442266
74.215554	2890.206012	21.447283
74.394028	2888.656310	21.452301
74.412213	2889.920770	21.457319
74.270572	2889.470219	21.462336
74.343631	2893.346666	21.467354
74.795971	2908.493890	21.472371
75.107938	2904.567957	21.477389
75.078426	2913.702757	21.482407
75.350602	2909.814909	21.487424
75.439920	2909.459590	21.492442
75.276145	2907.475966	21.497459
75.552594	2908.591356	21.502477
75.170517	2900.403225	21.507495
75.027016	2895.757373	21.512512
75.379930	2901.518344	21.517530
75.404958	2899.746392	21.522547
75.450894	2900.406997	21.527565
75.493080	2906.110358	21.532583
75.236281	2902.572328	21.537600
75.786759	2898.778569	21.542618
75.514583	2907.062925	21.547635
75.714237	2924.751025	21.552653
76.137923	2929.124586	21.557671
76.091053	2935.869165	21.562688
76.252439	2926.103508	21.567706
75.907906	2932.119358	21.572723
76.434184	2923.552441	21.577741
76.222338	2922.993425	21.582759
76.431598	2931.547710	21.587776
76.378036	2923.245717	21.592794
76.059229	2944.160493	21.597811
76.892296	2955.651907	21.602829
76.936345	2955.663954	21.607847
76.792334	2966.451344	21.612864
77.249445	2960.673652	21.617882
76.581741	2964.118398	21.622899
76.814169	2959.568560	21.627917
76.860957	2961.168869	21.632935
76.781972	2954.407811	21.637952
77.037909	2968.752507	21.642970
77.431242	2986.601931	21.647987
77.394165	2978.826751	21.653005
77.275126	2987.482675	21.658023
77.571656	2988.463239	21.663040
77.478487	2979.600009	21.668058
77.659777	2984.948447	21.673075
77.699343	2978.683540	21.678093
77.555773	2989.757511	21.683111
77.729089	2999.537574	21.688128
77.864313	3007.096593	21.693146
77.843016	3012.393933	21.698163
78.241693	3024.062059	21.703181
78.054779	3016.966452	21.708199
78.314476	3015.096569	21.713216
78.146207	3007.165129	21.718234
78.212532	3018.059471	21.723251
78.438753	3028.656061	21.728269
78.605334	3033.975847	21.733287
79.000127	3028.897879	21.738304
79.070620	3021.362369	21.743322
78.777104	3033.916839	21.748339
78.894174	3022.120486	21.753357
79.259573	3023.323921	21.758375
79.144091	3022.444588	21.763392
79.458371	3017.575642	21.768410
79.511983	3018.403500	21.773427
79.348568	3014.911798	21.778445
79.551439	3019.444793	21.783463
79.245509	3011.594812	21.788480
79.595472	3013.551654	21.793498
79.634291	3032.010273	21.798515
79.353900	3038.385654	21.803533
79.762672	3044.010253	21.808551
79.601881	3053.439337	21.813568
79.966930	3042.741379	21.818586
79.978039	3047.076194	21.823603
80.186333	3039.887575	21.828621
80.251055	3048.748560	21.833639
79.882694	3066.944691	21.838656
80.419591	3068.450471	21.843674
80.321731	3065.734981	21.848691
80.482320	3069.935591	21.853709
80.511613	3075.093068	21.858727
80.460761	3068.421011	21.863744
80.618570	3074.602577	21.868762
80.525359	3097.043336	21.873779
80.847650	3091.198936	21.878797
81.167557	3094.387256	21.883815
81.137086	3103.062047	21.888832
81.286605	3091.518167	21.893850
81.386852	3093.736467	21.898867
81.494598	3091.925990	21.903885
81.560202	3091.162351	21.908903
81.604457	3098.835305	21.913920
81.677911	3092.234790	21.918938
81.400554	3102.297041	21.923955
81.847351	3115.989740	21.928973
82.173637	3123.223844	21.933991
81.863069	3126.537041	21.939008
82.295500	3128.523948	21.944026
81.939039	3125.177188	21.949043
82.388159	3119.731501	21.954061
82.190304	3111.988782	21.959079
82.206044	3109.945090	21.964096
82.321129	3113.912674	21.969114
82.037652	3128.781915	21.974131
82.465904	3121.798593	21.979149
82.489059	3134.661372	21.984167
82.648924	3145.699778	21.989184
82.480695	3144.715775	21.994202
82.949441	3150.024548	21.999219
83.027246	3145.120696	22.004237
83.122327	3141.779882	22.009255
83.158405	3146.859086	22.014272
83.310592	3136.375856	22.019290
82.981595	3144.973316	22.024307
83.322131	3140.502780	22.029325
83.595982	3155.457732	22.034343
83.443392	3164.251606	22.039360
84.085829	3166.862863	22.044378
83.587971	3169.885790	22.049395
83.537915	3165.194460	22.054413
83.895859	3158.580672	22.059431
83.783572	3165.607074	22.064448
84.109579	3155.097807	22.069466
84.023326	3160.299643	22.074483
84.117603	3156.900291	22.079501
84.375950	3161.554864	22.084519
84.269697	3184.942882	22.089536
84.479886	3179.353254	22.094554
84.499737	3185.427774	22.099571
84.502171	3190.473583	22.104589
84.880669	3188.426119	22.109607
84.630573	3193.201508	22.114624
84.544856	3188.025871	22.119642
84.467741	3191.176003	22.124659
85.068658	3207.287204	22.129677
85.072665	3215.368889	22.134695
84.971007	3220.318152	22.139712
85.114093	3204.817772	22.144730
84.760102	3214.297449	22.149747
84.961298	3222.334674	22.154765
85.626342	3228.322065	22.159783
85.440285	3241.593627	22.164800
85.859808	3237.008399	22.169818
85.951689	3237.560614	22.174835
85.953509	3234.928600	22.179853
86.086823	3236.785504	22.184871
86.017003	3239.722606	22.189888
86.379047	3246.352361	22.194906
86.415697	3254.390468	22.199923
86.587297	3259.451206	22.204941
86.694620	3265.619552	22.209959
86.755471	3262.815143	22.214976
86.614637	3254.112027	22.219994
86.890101	3255.791050	22.225011
86.926994	3258.041913	22.230029
87.325307	3254.674884	22.235047
87.150813	3254.567197	22.240064
87.329683	3254.352176	22.245082
87.269538	3249.005338	22.250099
87.237408	3255.410572	22.255117
87.712422	3247.735524	22.260135
87.303168	3247.845073	22.265152
87.686567	3245.714499	22.270170
87.634072	3249.500002	22.275187
87.385522	3246.505464	22.280205
87.959266	3239.083784	22.285223
87.809307	3241.335660	22.290240
87.780299	3249.704354	22.295258
87.672810	3252.966232	22.300275
87.669527	3272.412127	22.305293
87.977165	3274.762666	22.310311
87.691784	3287.719183	22.315328
87.963848	3288.175810	22.320346
87.974501	3302.449212	22.325363
88.119089	3313.050457	22.330381
88.443119	3317.664670	22.335399
88.330788	3316.144966	22.340416
88.576375	3321.332465	22.345434
88.753401	3334.753063	22.350451
88.831294	3335.140651	22.355469
89.310928	3343.108210	22.360487
89.357753	3344.341190	22.365504
89.213999	3337.507217	22.370522
89.259161	3334.244714	22.375539
89.234663	3335.461547	22.380557
89.613204	3326.989355	22.385575
89.213074	3335.265985	22.390592
89.398487	3337.256022	22.395610
89.660880	3338.661204	22.400627
89.805328	3363.824709	22.405645
89.637459	3355.907200	22.410663
89.834007	3360.794531	22.415680
89.871947	3356.996153	22.420698
90.213824	3357.211276	22.425715
90.208276	3365.106017	22.430733
90.438763	3359.060553	22.435751
90.246808	3380.941236	22.440768
90.484698	3388.548408	22.445786
90.661240	3387.403353	22.450803
90.456945	3388.128251	22.455821
90.635600	3386.330411	22.460839
90.683629	3394.985672	22.465856
90.935055	3393.880192	22.470874
91.132456	3411.823971	22.475891
90.843871	3407.309875	22.480909
91.036173	3402.372416	22.485927
91.136044	3399.113047	22.490944
91.303802	3400.118898	22.495962
91.478917	3407.830973	22.500979
91.647216	3423.639974	22.505997
91.885479	3429.410284	22.511015
91.954378	3438.006595	22.516032
92.147887	3432.198749	22.521050
92.139954	3425.534001	22.526067
92.073785	3431.542930	22.531085
92.357168	3428.889461	22.536103
92.120019	3432.522491	22.541120
92.171410	3425.242734	22.546138
92.381023	3431.699755	22.551155
92.607544	3446.334834	22.556173
92.775400	3446.875659	22.561191
92.707040	3457.478793	22.566208
92.781067	3451.930515	22.571226
92.784174	3452.449794	22.576243
92.944979	3462.079446	22.581261
92.698545	3446.303127	22.586279
92.823419	3467.331771	22.591296
93.117082	3479.393263	22.596314
93.242540	3479.451681	22.601331
93.167746	3483.862265	22.606349
93.369571	3483.948595	22.611367
93.229207	3504.174651	22.616384
93.505484	3510.059183	22.621402
93.687484	3510.214157	22.626419
93.796258	3512.276756	22.631437
94.227111	3512.238540	22.636455
94.147016	3509.377100	22.641472
94.327849	3524.691157	22.646490
94.346947	3530.950997	22.651507
94.749369	3529.674032	22.656525
95.054842	3531.179986	22.661543
94.697947	3537.057937	22.666560
95.190258	3524.568684	22.671578
95.085331	3521.069939	22.676595
94.962592	3525.110869	22.681613
95.327932	3510.515624	22.686631
95.383207	3502.454387	22.691648
95.042585	3498.660382	22.696666
95.395608	3504.640485	22.701683
94.896600	3511.904717	22.706701
95.250287	3514.646141	22.711719
95.463317	3506.686355	22.716736
95.397217	3518.009321	22.721754
95.553097	3507.685486	22.726771
95.682156	3523.334925	22.731789
95.492201	3532.930169	22.736807
95.477995	3543.102297	22.741824
95.780246	3551.085159	22.746842
95.881762	3544.380189	22.751859
95.672765	3572.624965	22.756877
96.245069	3577.312729	22.761895
96.225519	3586.654171	22.766912
96.336495	3573.268059	22.771930
96.888528	3578.382066	22.776947
96.722116	3596.623334	22.781965
97.063493	3598.573012	22.786983
97.091314	3594.168302	22.792000
97.460487	3606.612321	22.797018
97.488801	3603.373814	22.802035
97.196633	3597.895174	22.807053
97.385646	3594.444605	22.812071
97.535658	3598.435273	22.817088
97.459618	3594.209592	22.822106
97.846702	3583.662757	22.827123
97.533216	3593.265891	22.832141
97.612206	3586.258296	22.837159
97.936202	3599.880012	22.842176
98.165555	3619.164182	22.847194
98.242364	3623.750909	22.852211
98.218331	3623.943150	22.857229
98.427207	3624.195263	22.862247
98.421523	3625.918911	22.867264
98.253590	3624.780083	22.872282
98.563185	3620.049935	22.877299
98.611975	3642.540020	22.882317
98.802611	3643.965382	22.887335
99.004971	3651.223009	22.892352
98.946085	3648.424576	22.897370
98.723542	3642.348491	22.902387
98.971679	3644.650271	22.907405
99.047581	3658.902169	22.912423
99.268401	3675.175231	22.917440
99.427782	3676.769965	22.922458
99.717002	3679.320098	22.927475
99.723411	3676.111979	22.932493
99.730341	3666.694313	22.937511
100.042538	3670.141543	22.942528
99.858207	3694.164589	22.947546
100.169244	3680.558622	22.952563
100.212504	3700.587577	22.957581
99.982414	3689.362839	22.962599
100.565351	3686.890073	22.967616
100.423183	3699.957485	22.972634
100.783001	3690.876702	22.977651
100.596247	3701.991008	22.982669
100.446356	3716.557546	22.987687
101.105718	3717.218599	22.992704
101.093656	3715.532628	22.997722
101.235511	3726.148387	23.002739
101.111522	3720.279605	23.007757
101.221147	3723.930490	23.012775
101.557398	3724.415092	23.017792
101.131334	3721.247464	23.022810
101.763784	3735.905378	23.027827
101.929906	3742.594957	23.032845
102.153178	3748.462368	23.037863
102.161003	3748.847787	23.042880
102.380531	3754.331911	23.047898
102.409712	3739.258185	23.052915
102.445004	3741.389289	23.057933
102.121386	3738.911876	23.062951
102.500914	3740.785562	23.067968
102.371516	3746.937381	23.072986
102.694372	3737.429956	23.078003
102.729171	3733.931652	23.083021
102.322601	3733.106775	23.088039
102.864676	3735.165779	23.093056
102.469199	3752.606462	23.098074
102.592210	3764.034925	23.103091
102.459513	3775.503373	23.108109
102.722851	3775.188916	23.113127
102.945206	3787.230953	23.118144
102.890474	3805.238588	23.123162
103.359117	3807.602320	23.128179
103.895924	3815.415755	23.133197
103.752675	3818.957725	23.138215
104.261565	3813.591288	23.143232
103.839680	3819.704545	23.148250
103.932193	3808.792891	23.153267
104.144960	3821.334248	23.158285
104.054407	3845.788517	23.163303
104.432917	3849.530757	23.168320
104.471398	3843.962238	23.173338
104.707140	3844.014211	23.178355
104.722215	3839.791883	23.183373
104.502850	3844.830133	23.188391
104.930685	3854.507952	23.193408
104.997313	3869.423876	23.198426
105.328044	3869.674718	23.203443
105.200043	3875.937789	23.208461
105.231707	3877.509984	23.213479
105.400785	3868.247659	23.218496
105.515243	3899.654095	23.223514
105.745696	3896.243062	23.228531
105.783300	3898.699835	23.233549
105.753503	3896.462370	23.238567
106.153202	3893.932893	23.243584
106.076095	3899.288994	23.248602
105.903242	3919.303611	23.253619
106.137399	3925.268120	23.258637
106.221083	3920.402035	23.263655
106.734530	3914.520168	23.268672
106.829402	3922.355643	23.273690
106.995774	3922.615194	23.278707
107.351161	3926.328599	23.283725
107.176656	3926.205944	23.288743
107.368681	3930.644138	23.293760
107.689062	3940.206319	23.298778
107.978986	3930.550665	23.303795
107.750440	3917.927272	23.308813
107.646176	3910.224179	23.313831
107.720635	3914.870838	23.318848
107.989359	3933.511384	23.323866
107.995312	3935.139424	23.328883
108.531026	3930.921824	23.333901
108.189812	3933.084581	23.338919
108.168835	3929.282038	23.343936
108.049932	3935.786181	23.348954
108.069470	3929.585637	23.353971
108.231407	3932.421887	23.358989
108.298477	3951.454951	23.364007
108.631647	3951.527412	23.369024
108.171189	3959.949022	23.374042
108.607485	3958.733355	23.379059
108.595780	3967.984737	23.384077
108.712571	3991.396485	23.389095
108.831156	3986.900641	23.394112
109.050127	3994.835701	23.399130
109.055026	3988.812780	23.404147
109.195584	4014.478444	23.409165
108.958676	4023.767934	23.414183
109.528880	4013.212937	23.419200
109.379651	4034.736222	23.424218
109.697843	4049.533880	23.429235
109.847633	4035.703086	23.434253
109.926545	4043.489681	23.439271
110.374177	4058.267491	23.444288
110.621427	4069.592916	23.449306
110.981433	4071.421049	23.454323
111.267383	4065.563408	23.459341
111.215980	4075.655412	23.464359
111.677991	4062.275338	23.469376
111.359095	4048.150424	23.474394
111.343641	4031.834011	23.479411
111.684122	4028.809517	23.484429
111.584881	4030.710535	23.489447
111.453976	4024.786476	23.494464
111.819192	4037.535872	23.499482
111.776377	4054.065217	23.504499
111.709936	4052.183850	23.509517
111.456819	4057.011582	23.514535
111.907380	4062.574902	23.519552
111.845040	4064.685596	23.524570
112.149510	4088.483014	23.529587
112.409706	4088.488807	23.534605
112.512273	4088.815233	23.539623
112.806905	4076.184233	23.544640
112.530963	4086.257508	23.549658
112.546931	4087.060550	23.554675
112.933722	4088.488913	23.559693
112.897098	4109.986569	23.564711
113.171137	4109.107255	23.569728
113.425247	4113.552547	23.574746
113.031693	4120.388901	23.579763
113.251990	4105.916350	23.584781
113.440994	4109.521107	23.589799
113.885490	4121.094270	23.594816
113.849283	4132.711595	23.599834
113.646120	4136.142671	23.604851
114.133293	4138.217515	23.609869
113.630166	4134.100203	23.614887
114.230425	4148.500804	23.619904
114.445412	4160.888499	23.624922
114.544956	4165.478315	23.629939
114.889527	4161.051320	23.634957
114.629757	4168.617633	23.639975
114.671875	4158.179116	23.644992
114.856260	4163.044694	23.650010
114.996854	4181.648080	23.655027
115.369149	4168.059112	23.660045
115.179476	4178.151239	23.665063
115.130834	4169.708376	23.670080
115.295991	4184.577178	23.675098
115.592807	4187.138740	23.680115
116.034064	4196.931105	23.685133
115.965165	4206.107044	23.690151
116.356404	4202.401563	23.695168
116.397163	4200.081101	23.700186
116.537944	4202.778755	23.705203
116.181413	4199.426257	23.710221
116.085477	4208.750792	23.715239
116.350524	4193.443845	23.720256
116.629819	4198.322070	23.725274
116.208182	4198.909338	23.730291
116.518763	4215.374827	23.735309
116.626284	4220.316940	23.740327
116.935220	4216.955058	23.745344
117.001083	4240.373248	23.750362
116.911687	4246.484382	23.755379
117.435548	4250.702342	23.760397
117.355921	4264.333586	23.765415
117.369694	4260.171606	23.770432
117.889481	4274.071389	23.775450
117.886732	4283.464805	23.780467
118.309379	4284.793534	23.785485
118.252504	4291.692347	23.790503
118.351942	4275.401546	23.795520
118.234494	4279.372884	23.800538
118.170966	4283.278592	23.805555
118.685065	4289.857631	23.810573
118.539710	4298.802935	23.815591
118.686226	4307.481771	23.820608
118.923794	4306.072174	23.825626
118.886292	4317.419725	23.830643
119.138382	4321.751219	23.835661
119.179958	4330.311199	23.840679
119.501214	4337.308081	23.845696
119.584896	4335.004118	23.850714
119.420382	4348.423466	23.855731
119.503953	4357.450605	23.860749
119.678994	4370.423920	23.865767
119.765409	4368.762131	23.870784
120.234916	4369.571210	23.875802
120.062019	4396.328949	23.880819
120.304700	4396.422698	23.885837
120.448447	4400.053129	23.890855
120.795248	4383.974060	23.895872
120.982660	4395.105656	23.900890
120.995548	4399.938276	23.905907
121.007373	4407.658981	23.910925
121.098822	4416.547030	23.915943
121.261753	4417.259602	23.920960
121.418273	4415.249133	23.925978
120.965127	4414.771357	23.930995
121.638822	4431.786509	23.936013
121.798372	4438.896840	23.941031
121.946045	4434.029058	23.946048
122.196886	4438.027661	23.951066
121.956652	4437.342161	23.956083
122.462682	4424.913717	23.961101
122.591691	4441.309490	23.966119
122.741222	4458.181495	23.971136
122.981123	4456.754173	23.976154
122.743834	4464.679174	23.981171
123.374175	4464.801668	23.986189
123.349947	4464.646645	23.991207
122.991735	4472.109695	23.996224
123.447418	4449.231786	24.001242
122.991667	4463.216081	24.006259
123.504159	4452.481338	24.011277
123.686761	4468.354788	24.016295
123.908718	4478.811313	24.021312
124.084885	4476.054930	24.026330
123.883168	4475.363050	24.031347
123.950222	4474.658958	24.036365
123.913830	4484.641634	24.041383
124.141013	4488.136989	24.046400
124.359005	4493.759449	24.051418
124.409441	4516.004014	24.056435
124.632414	4517.268169	24.061453
124.506688	4508.582722	24.066471
124.694216	4508.384761	24.071488
124.710215	4518.709242	24.076506
124.884369	4533.673754	24.081523
124.773910	4538.209458	24.086541
124.919897	4555.670452	24.091559
125.298349	4564.037749	24.096576
125.298232	4565.296318	24.101594
125.663409	4578.470651	24.106611
125.840856	4578.880771	24.111629
126.044637	4586.904490	24.116647
125.922393	4593.351180	24.121664
126.421043	4587.977124	24.126682
126.387036	4588.605754	24.131699
126.469812	4592.145519	24.136717
126.558499	4602.035105	24.141735
127.003687	4610.061394	24.146752
127.365477	4606.370147	24.151770
126.695862	4621.018455	24.156787
127.626916	4609.436205	24.161805
127.616292	4613.222979	24.166823
127.536020	4619.214613	24.171840
127.800169	4610.077082	24.176858
127.730988	4618.078283	24.181875
128.103212	4631.427118	24.186893
128.289023	4630.966398	24.191911
128.358493	4631.388886	24.196928
128.541777	4631.249905	24.201946
128.202169	4638.571344	24.206963
128.608584	4629.134605	24.211981
128.466121	4631.772911	24.216999
128.352044	4632.858191	24.222016
128.945290	4654.138108	24.227034
128.934239	4663.992269	24.232051
129.000788	4664.057692	24.237069
129.232312	4666.087521	24.242087
129.192373	4668.369422	24.247104
129.309882	4677.324972	24.252122
129.292314	4684.615950	24.257139
129.529008	4678.494532	24.262157
129.951009	4696.791256	24.267175
130.042800	4714.737084	24.272192
130.466523	4715.756953	24.277210
130.306269	4718.880203	24.282227
130.496179	4714.125838	24.287245
130.439063	4718.515727	24.292263
130.399591	4723.276784	24.297280
130.942187	4727.236607	24.302298
130.772377	4738.140135	24.307315
131.058104	4741.920401	24.312333
131.283165	4739.078697	24.317351
130.924571	4747.731937	24.322368
131.167925	4757.992942	24.327386
131.425727	4771.556943	24.332403
131.868750	4773.954211	24.337421
131.650996	4774.265170	24.342439
131.938145	4794.708381	24.347456
132.354638	4794.571741	24.352474
132.277088	4795.160335	24.357491
132.111324	4793.554431	24.362509
132.680577	4795.720524	24.367527
132.585013	4814.353522	24.372544
132.565455	4816.048489	24.377562
132.812772	4825.730813	24.382579
132.856890	4830.125235	24.387597
133.110878	4818.219415	24.392615
132.853841	4831.170143	24.397632
133.394559	4836.710153	24.402650
133.305759	4855.938265	24.407667
133.673603	4858.082584	24.412685
133.825938	4852.545262	24.417703
133.466132	4861.432671	24.422720
134.067829	4870.894110	24.427738
134.004162	4879.148126	24.432755
134.318645	4881.781698	24.437773
134.507536	4875.070358	24.442791
134.616475	4889.361614	24.447808
134.916620	4894.905249	24.452826
135.057511	4907.346756	24.457843
135.183153	4904.941256	24.462861
135.201784	4905.220955	24.467879
135.288812	4896.904088	24.472896
135.493494	4889.229299	24.477914
135.271162	4906.994236	24.482931
135.237258	4916.712940	24.487949
135.709232	4926.605426	24.492967
135.864520	4924.250143	24.497984
135.897605	4931.650197	24.503002
136.100438	4957.713478	24.508019
136.175457	4962.169764	24.513037
136.409442	4957.936487	24.518055
136.654067	4976.169972	24.523072
137.088741	4970.827645	24.528090
137.066357	4978.080179	24.533107
137.067474	4990.226716	24.538125
137.197708	4976.720449	24.543143
137.135350	4980.756873	24.548160
137.504983	4986.900976	24.553178
137.575642	4995.732940	24.558195
137.639198	5002.889349	24.563213
137.668766	5002.543484	24.568231
137.983821	5014.206473	24.573248
138.059501	5021.490045	24.578266
138.303258	5032.751378	24.583283
138.332153	5027.365169	24.588301
138.811699	5028.988549	24.593319
138.510591	5037.263058	24.598336
138.694564	5046.621288	24.603354
138.837915	5051.193085	24.608371
138.886956	5055.786799	24.613389
139.006039	5065.876414	24.618407
139.080990	5081.281587	24.623424
139.571497	5082.882681	24.628442
139.609319	5080.556275	24.633459
140.013693	5104.551340	24.638477
140.127294	5102.536865	24.643495
139.829822	5116.779844	24.648512
140.232264	5107.985352	24.653530
140.858467	5110.650048	24.658547
140.649472	5115.851981	24.663565
140.993718	5124.116557	24.668583
140.644711	5142.770641	24.673600
141.052606	5135.921333	24.678618
141.156399	5142.070921	24.683635
140.700448	5140.339760	24.688653
141.282251	5152.556458	24.693671
141.469696	5163.037268	24.698688
141.627333	5153.304324	24.703706
142.052866	5156.729974	24.708723
142.048866	5162.277594	24.713741
142.307914	5158.670964	24.718759
142.153127	5189.850088	24.723776
142.552263	5194.683582	24.728794
142.660631	5187.843678	24.733811
142.566659	5184.285252	24.738829
143.322664	5188.346113	24.743847
142.766894	5187.315091	24.748864
143.057638	5183.205458	24.753882
142.914335	5184.226307	24.758899
142.971929	5208.392358	24.763917
143.570816	5205.580825	24.768935
143.403618	5212.508545	24.773952
143.560914	5217.964110	24.778970
143.748849	5224.517216	24.783987
143.573006	5242.311062	24.789005
143.658823	5239.023713	24.794023
144.149677	5257.979137	24.799040
143.747864	5269.566473	24.804058
144.275699	5271.719016	24.809075
144.308557	5282.017578	24.814093
144.547357	5297.295812	24.819111
144.875243	5309.310522	24.824128
145.447946	5320.349056	24.829146
145.642012	5328.140063	24.834163
145.723379	5332.235477	24.839181
146.233996	5318.066586	24.844199
145.982066	5328.352474	24.849216
146.218190	5316.433486	24.854234
146.309825	5318.046301	24.859251
146.200643	5336.254512	24.864269
146.418094	5326.157145	24.869287
146.407497	5346.484978	24.874304
146.796931	5352.638549	24.879322
146.878086	5348.443073	24.884339
146.499411	5356.856605	24.889357
146.943474	5365.074067	24.894375
147.040788	5376.263807	24.899392
146.979543	5380.201699	24.904410
147.474253	5387.590120	24.909427
147.441239	5407.119189	24.914445
148.064802	5405.055685	24.919463
148.026070	5416.186069	24.924480
148.178417	5411.446379	24.929498
148.523320	5417.942862	24.934515
148.653591	5430.706304	24.939533
149.170872	5412.673880	24.944551
148.936601	5416.129282	24.949568
148.521490	5427.118004	24.954586
148.832890	5424.097277	24.959603
148.824748	5434.167238	24.964621
149.155219	5441.961708	24.969639
149.274541	5448.031661	24.974656
149.294702	5456.998259	24.979674
149.666894	5469.831941	24.984691
149.656379	5474.567166	24.989709
149.918415	5478.890248	24.994727
150.224660	5501.545143	24.999744
150.038767	5508.244534	25.004762
150.778322	5506.343748	25.009779
150.184717	5507.743972	25.014797
150.784877	5533.021772	25.019815
150.710847	5530.337348	25.024832
150.840922	5536.063737	25.029850
151.266910	5549.042159	25.034867
151.294369	5560.984725	25.039885
151.722172	5556.543565	25.044903
151.905532	5561.751567	25.049920
151.878151	5570.830852	25.054938
152.265312	5576.461135	25.059955
152.261824	5582.828708	25.064973
152.635787	5576.243950	25.069991
152.906795	5581.172813	25.075008
153.001113	5584.787289	25.080026
153.124342	5579.998025	25.085043
152.912932	5586.124364	25.090061
153.079594	5573.258175	25.095079
153.178755	5578.623466	25.100096
153.317733	5598.612607	25.105114
153.721297	5606.983395	25.110131
153.254321	5615.684980	25.115149
153.726909	5618.027080	25.120167
153.768032	5617.561149	25.125184
153.893889	5643.397304	25.130202
154.203719	5632.247176	25.135219
153.902490	5640.503903	25.140237
153.936416	5648.549200	25.145255
154.357320	5668.923360	25.150272
154.511416	5678.765776	25.155290
154.972654	5691.454155	25.160307
154.492980	5703.123219	25.165325
154.762557	5724.418011	25.170343
155.130974	5725.926761	25.175360
155.299259	5741.380922	25.180378
156.041677	5752.083709	25.185395
155.731948	5752.801354	25.190413
155.915172	5748.653457	25.195431
156.191532	5769.402163	25.200448
156.451368	5780.900803	25.205466
157.052030	5777.226449	25.210483
157.277175	5781.646298	25.215501
157.056527	5775.767938	25.220519
157.244763	5781.091772	25.225536
157.098245	5804.348185	25.230554
157.051620	5807.022013	25.235571
157.344931	5816.124741	25.240589
157.767705	5831.605379	25.245607
157.927760	5841.832840	25.250624
157.939336	5848.978549	25.255642
158.422759	5836.040800	25.260659
158.122574	5846.691013	25.265677
158.222349	5854.641238	25.270695
158.446464	5860.145034	25.275712
158.568592	5864.526830	25.280730
159.137583	5868.183286	25.285747
158.896558	5891.580706	25.290765
159.315951	5878.859090	25.295783
159.759085	5899.382665	25.300800
159.698562	5913.543809	25.305818
160.080876	5910.598677	25.310835
160.450681	5910.340595	25.315853
160.375628	5906.009374	25.320871
160.518801	5909.764694	25.325888
160.754608	5912.230318	25.330906
160.859339	5903.583130	25.335923
160.768439	5926.451672	25.340941
160.597950	5933.874087	25.345959
161.058970	5932.724286	25.350976
160.654539	5954.277476	25.355994
161.293418	5961.617885	25.361011
161.120633	5969.647161	25.366029
161.401758	5986.380876	25.371047
161.811610	5991.155349	25.376064
161.927198	6002.099921	25.381082
162.387908	6001.266790	25.386099
162.425610	6027.517491	25.391117
162.731394	6024.273899	25.396135
162.809730	6018.461728	25.401152
162.606119	6024.393977	25.406170
163.070127	6027.498403	25.411187
162.953358	6035.655485	25.416205
163.057465	6052.196467	25.421223
163.567398	6048.712714	25.426240
163.152676	6056.504847	25.431258
163.867609	6059.944219	25.436275
164.128145	6078.375616	25.441293
164.036414	6076.027194	25.446311
164.418621	6068.474456	25.451328
164.348028	6080.506897	25.456346
164.404453	6087.959550	25.461363
164.898005	6101.168256	25.466381
165.035491	6104.933228	25.471399
165.275663	6104.782458	25.476416
165.114641	6113.484855	25.481434
165.465130	6128.954125	25.486451
165.476672	6129.294092	25.491469
165.328871	6135.507776	25.496487
165.886563	6158.073151	25.501504
165.907021	6170.422965	25.506522
166.004821	6172.599578	25.511539
166.089902	6169.008922	25.516557
166.212686	6188.513161	25.521575
166.599564	6193.825513	25.526592
166.791921	6218.121234	25.531610
166.850977	6227.648136	25.536627
167.133903	6229.864993	25.541645
167.337553	6244.546640	25.546663
168.060630	6248.271405	25.551680
167.515605	6246.464284	25.556698
167.903408	6244.957974	25.561715
168.164896	6265.146637	25.566733
168.318221	6287.181332	25.571751
168.799436	6277.156261	25.576768
168.580651	6283.103721	25.581786
168.851717	6274.428005	25.586803
169.330044	6298.924609	25.591821
169.069624	6302.563324	25.596839
169.609033	6301.656503	25.601856
169.307436	6304.847571	25.606874
169.422356	6300.545437	25.611891
169.945492	6321.584819	25.616909
169.754424	6324.129846	25.621927
169.857917	6321.033105	25.626944
170.174430	6357.215961	25.631962
170.301097	6361.272637	25.636979
170.153391	6368.292937	25.641997
170.527363	6390.303059	25.647015
170.606657	6386.233640	25.652032
171.130670	6405.311768	25.657050
171.050852	6414.732602	25.662067
171.315975	6411.079790	25.667085
171.457438	6440.407058	25.672103
171.981947	6447.732763	25.677120
172.201701	6455.248340	25.682138
172.185822	6448.172479	25.687156
172.333858	6461.001550	25.692173
172.183086	6475.375836	25.697191
172.866610	6466.334788	25.702208
172.930667	6487.586659	25.707226
173.346248	6498.239313	25.712244
173.524990	6509.043819	25.717261
173.594858	6505.701351	25.722279
173.952810	6506.702307	25.727296
173.977441	6499.652010	25.732314
173.907103	6526.126212	25.737332
174.261359	6525.550914	25.742349
174.083189	6535.977385	25.747367
174.475259	6522.607610	25.752384
174.635509	6535.754504	25.757402
174.593490	6554.090044	25.762420
174.896442	6553.097910	25.767437
175.109130	6554.419074	25.772455
175.402542	6550.819046	25.777472
175.216802	6549.747927	25.782490
175.287433	6574.916583	25.787508
175.656114	6571.946021	25.792525
175.699454	6596.678146	25.797543
175.486068	6603.043860	25.802560
175.661135	6616.869684	25.807578
175.904275	6638.721441	25.812596
176.215538	6643.163508	25.817613
176.449898	6668.590334	25.822631
177.184651	6665.690687	25.827648
177.036114	6674.598475	25.832666
177.235633	6690.294141	25.837684
177.751806	6690.819952	25.842701
177.455558	6700.557192	25.847719
177.739650	6708.371785	25.852736
178.271996	6729.373955	25.857754
178.213317	6727.175131	25.862772
178.385328	6743.243240	25.867789
178.657045	6747.002684	25.872807
178.723852	6748.620546	25.877824
178.861907	6757.283231	25.882842
179.400662	6769.695782	25.887860
179.471091	6779.702392	25.892877
179.456988	6779.027389	25.897895
179.894639	6775.404218	25.902912
179.962978	6789.853572	25.907930
180.252541	6806.930178	25.912948
180.698042	6795.882801	25.917965
180.204401	6803.562337	25.922983
180.541505	6817.032267	25.928000
180.793725	6835.823522	25.933018
180.783211	6846.616270	25.938036
181.021956	6847.705512	25.943053
181.046155	6866.670819	25.948071
181.610555	6866.395476	25.953088
181.804741	6870.722300	25.958106
181.782670	6895.357023	25.963124
182.236083	6891.148345	25.968141
181.799180	6902.492199	25.973159
182.535103	6913.326823	25.978176
182.640898	6930.839634	25.983194
182.866136	6927.835257	25.988212
183.545317	6933.575217	25.993229
183.416868	6961.642974	25.998247
183.649524	6954.417830	26.003264
183.864410	6965.823956	26.008282
183.475361	6963.988561	26.013300
183.848644	6971.779855	26.018317
184.240660	6979.579078	26.023335
184.530670	6980.358165	26.028352
184.298873	6982.223979	26.033370
184.242592	7000.953080	26.038388
184.858913	7008.635628	26.043405
184.642856	7013.927567	26.048423
185.330512	7038.259908	26.053440
185.416511	7041.108903	26.058458
185.273484	7037.350234	26.063476
185.665193	7057.263144	26.068493
186.017380	7076.926628	26.073511
186.023910	7073.060485	26.078528
186.365708	7085.817024	26.083546
186.050375	7090.155009	26.088564
186.668098	7093.171189	26.093581
186.977889	7101.789089	26.098599
187.076943	7119.311889	26.103616
187.391619	7123.879556	26.108634
187.314075	7128.406609	26.113652
187.170273	7129.808110	26.118669
187.574730	7137.751073	26.123687
187.742080	7153.399750	26.128704
187.955517	7160.948215	26.133722
188.142932	7176.500647	26.138740
188.626931	7190.894941	26.143757
188.832694	7190.294584	26.148775
188.431710	7195.359627	26.153792
188.922005	7201.810725	26.158810
188.976062	7212.226761	26.163828
189.663645	7213.249597	26.168845
189.550014	7238.000044	26.173863
189.608295	7235.635278	26.178880
189.921474	7242.478049	26.183898
190.189365	7268.492623	26.188916
190.242397	7261.639721	26.193933
190.632181	7279.543852	26.198951
190.442430	7290.425651	26.203968
190.757712	7303.814540	26.208986
191.128620	7303.743730	26.214004
191.640758	7305.981084	26.219021
191.232408	7318.210588	26.224039
191.707122	7331.054020	26.229056
191.981449	7347.800541	26.234074
191.851259	7348.509793	26.239092
192.371053	7364.354752	26.244109
192.624951	7381.269316	26.249127
192.482984	7381.158961	26.254144
192.965016	7393.768865	26.259162
193.071908	7407.556254	26.264180
193.733710	7413.053511	26.269197
193.368997	7418.176421	26.274215
193.873950	7424.134454	26.279232
194.073869	7436.863565	26.284250
193.797998	7445.352545	26.289268
194.040431	7453.962097	26.294285
194.570685	7468.963386	26.299303
194.640361	7472.942349	26.304320
194.910466	7480.940811	26.309338
195.007331	7500.510820	26.314356
195.384678	7508.085878	26.319373
195.685994	7512.502270	26.324391
195.708054	7528.492811	26.329408
195.956804	7528.012931	26.334426
196.143649	7539.660421	26.339444
196.516298	7534.576428	26.344461
196.645017	7549.751396	26.349479
196.626018	7558.724091	26.354496
197.111588	7558.175072	26.359514
197.220928	7555.656869	26.364532
197.611507	7571.902310	26.369549
197.418057	7594.917837	26.374567
197.279715	7581.651532	26.379584
197.925794	7593.131660	26.384602
197.800707	7614.016988	26.389620
198.446541	7614.067656	26.394637
198.197025	7613.400083	26.399655
198.358317	7633.938700	26.404672
198.551436	7639.432497	26.409690
198.624765	7654.949146	26.414708
198.952091	7663.991384	26.419725
198.897239	7674.647097	26.424743
199.120821	7694.920265	26.429760
199.807790	7691.833790	26.434778
199.382871	7716.534901	26.439796
199.770029	7733.824783	26.444813
199.983153	7738.841103	26.449831
200.093010	7753.886267	26.454848
200.605715	7756.106265	26.459866
200.469984	7763.445792	26.464884
201.046670	7789.959128	26.469901
200.730780	7793.025245	26.474919
201.483803	7816.205784	26.479936
201.749228	7817.432466	26.484954
201.855782	7823.926083	26.489972
202.357665	7835.052158	26.494989
202.588977	7843.941037	26.500007
202.533745	7853.416153	26.505024
203.200111	7859.873034	26.510042
203.233451	7881.426457	26.515060
203.899778	7877.257898	26.520077
203.559613	7881.843609	26.525095
203.530258	7883.056081	26.530112
203.785845	7884.838160	26.535130
203.884633	7905.014098	26.540148
203.929555	7904.552987	26.545165
204.194195	7921.970486	26.550183
204.320717	7931.551046	26.555200
204.642528	7942.904725	26.560218
204.755328	7973.915040	26.565236
204.885010	7972.805782	26.570253
205.503240	7986.009606	26.575271
205.081061	8001.273057	26.580288
205.713382	7999.029767	26.585306
205.834812	8020.156030	26.590324
206.064659	8033.185512	26.595341
206.094194	8043.915725	26.600359
206.300662	8054.403182	26.605376
206.715295	8064.227581	26.610394
207.042051	8087.557858	26.615412
207.505886	8094.143679	26.620429
207.523390	8110.499486	26.625447
207.025637	8127.638536	26.630464
208.186548	8125.801624	26.635482
208.265591	8140.006237	26.640500
208.319506	8142.191963	26.645517
208.728647	8146.945947	26.650535
209.009382	8163.120377	26.655552
209.369119	8163.765886	26.660570
209.337441	8171.208108	26.665588
209.471791	8163.351184	26.670605
210.000271	8188.135441	26.675623
209.850832	8188.955047	26.680640
210.318227	8200.686550	26.685658
210.495669	8204.112201	26.690676
210.795098	8213.502821	26.695693
210.893256	8217.570995	26.700711
210.982502	8223.657234	26.705728
211.108408	8212.163948	26.710746
211.188789	8246.357859	26.715764
211.399984	8238.207745	26.720781
211.661806	8259.275635	26.725799
211.741000	8275.645817	26.730816
212.119951	8276.222769	26.735834
212.130737	8298.930579	26.740852
212.677392	8311.345399	26.745869
212.885580	8325.780085	26.750887
212.775168	8338.292676	26.755904
213.183621	8338.841114	26.760922
213.152630	8344.605427	26.765940
213.480731	8370.544089	26.770957
213.809967	8368.442305	26.775975
213.878649	8373.782079	26.780992
214.025360	8390.432665	26.786010
214.036542	8398.023869	26.791028
214.389723	8412.607932	26.796045
214.959119	8423.760269	26.801063
214.806098	8433.827756	26.806080
215.126483	8436.048182	26.811098
215.294127	8459.432129	26.816116
215.586409	8460.361377	26.821133
215.932847	8467.778164	26.826151
216.084121	8493.791989	26.831168
216.394249	8481.563771	26.836186
216.838923	8494.726643	26.841204
217.025193	8517.332452	26.846221
217.358695	8510.851662	26.851239
217.122571	8525.266343	26.856256
217.455157	8529.745590	26.861274
217.423187	8541.775858	26.866292
217.378136	8557.196396	26.871309
217.850361	8567.545665	26.876327
217.872389	8582.155559	26.881344
218.349271	8592.630902	26.886362
218.790956	8607.937824	26.891380
218.746425	8616.505710	26.896397
218.916136	8636.923700	26.901415
219.391478	8640.164634	26.906432
219.458399	8657.269060	26.911450
219.515735	8682.834759	26.916468
219.840353	8683.919369	26.921485
220.357816	8696.731625	26.926503
220.146567	8713.014845	26.931520
220.489791	8720.210923	26.936538
220.868274	8734.768248	26.941556
221.065856	8754.599623	26.946573
221.413872	8759.482075	26.951591
221.167324	8777.877664	26.956608
221.771120	8785.922375	26.961626
222.065114	8812.992320	26.966644
222.073544	8810.714351	26.971661
222.605133	8824.788724	26.976679
222.368394	8851.132053	26.981696
222.962895	8843.911541	26.986714
223.177899	8863.354953	26.991732
223.238602	8867.549234	26.996749
223.653992	8882.514158	27.001767
223.670069	8907.418236	27.006784
223.704647	8905.566831	27.011802
223.787033	8933.225021	27.016820
224.086244	8943.622084	27.021837
225.276663	8956.764292	27.026855
225.358507	8957.804822	27.031872
225.876450	8959.863424	27.036890
225.907470	8959.256484	27.041908
226.404502	8976.089954	27.046925
226.389713	8982.030637	27.051943
226.877248	8987.730610	27.056960
227.061299	8978.137486	27.061978
226.989156	8992.483688	27.066996
227.270107	8986.840927	27.072013
227.260265	8985.127636	27.077031
227.106679	9013.904270	27.082048
227.407344	9015.406449	27.087066
227.590110	9030.736159	27.092084
227.912356	9047.084226	27.097101
228.205356	9040.100243	27.102119
228.062162	9075.466539	27.107136
228.284725	9074.692388	27.112154
228.828422	9085.448471	27.117172
228.759753	9104.261652	27.122189
229.079582	9099.227667	27.127207
228.946679	9121.394022	27.132224
229.335330	9133.497689	27.137242
229.765210	9140.889948	27.142260
229.440962	9159.569831	27.147277
230.007562	9179.505289	27.152295
230.024600	9197.051826	27.157312
230.228563	9225.260743	27.162330
230.729050	9219.969145	27.167348
230.863076	9253.790798	27.172365
231.432612	9252.373879	27.177383
231.310521	9279.374845	27.182400
231.626450	9291.107021	27.187418
231.667033	9310.313580	27.192436
232.155726	9331.832176	27.197453
232.388252	9350.273580	27.202471
232.542354	9358.467081	27.207488
232.985261	9381.872980	27.212506
233.173403	9394.013189	27.217524
233.775769	9415.141244	27.222541
233.835621	9420.470226	27.227559
234.048275	9434.562487	27.232576
234.163321	9451.834682	27.237594
234.732658	9454.885338	27.242612
234.813952	9472.879245	27.247629
235.205064	9475.851481	27.252647
235.273305	9489.052283	27.257664
235.650880	9502.325571	27.262682
235.832825	9518.117530	27.267700
235.808883	9526.756546	27.272717
236.347151	9545.616298	27.277735
236.576517	9555.134327	27.282752
236.485078	9573.342074	27.287770
237.037664	9579.286738	27.292788
237.279623	9591.107008	27.297805
237.350421	9598.361187	27.302823
237.685443	9611.017674	27.307840
237.915213	9630.617133	27.312858
237.927197	9633.006954	27.317876
238.173229	9654.292790	27.322893
238.571456	9657.187467	27.327911
238.717211	9677.078195	27.332928
238.985361	9685.915524	27.337946
238.860937	9704.637012	27.342964
239.300661	9726.350955	27.347981
239.525400	9743.524162	27.352999
239.604848	9762.724039	27.358016
240.290840	9776.210413	27.363034
240.483570	9790.347250	27.368052
240.233488	9809.906617	27.373069
240.993655	9814.562817	27.378087
240.996527	9835.226600	27.383104
241.190699	9858.988709	27.388122
241.468395	9870.439301	27.393140
241.931390	9886.263877	27.398157
242.069899	9897.514580	27.403175
242.462372	9919.831405	27.408192
242.897416	9932.216337	27.413210
243.513865	9943.868518	27.418228
243.397754	9955.415087	27.423245
243.853247	9951.340785	27.428263
243.786360	9962.659411	27.433280
243.613510	9984.065447	27.438298
244.152594	9981.145631	27.443316
244.080180	9998.284794	27.448333
244.466188	10004.078360	27.453351
245.001110	10024.382511	27.458368
245.016540	10033.677836	27.463386
245.385348	10039.367119	27.468404
245.611414	10062.201713	27.473421
246.235862	10060.951323	27.478439
245.899335	10074.253489	27.483456
246.285884	10087.530504	27.488474
246.450944	10093.181843	27.493492
246.273589	10119.971990	27.498509
246.819182	10122.522501	27.503527
246.987266	10142.899348	27.508544
247.250844	10162.513554	27.513562
247.786753	10177.506223	27.518580
247.536442	10191.972012	27.523597
247.778064	10207.995846	27.528615
248.351663	10231.783932	27.533632
248.344287	10248.670731	27.538650
248.564251	10269.905761	27.543668
248.729083	10288.034076	27.548685
249.242982	10301.916512	27.553703
249.603642	10312.624941	27.558720
249.763434	10330.093146	27.563738
250.057249	10352.887788	27.568756
250.168514	10379.417871	27.573773
250.391138	10388.170159	27.578791
250.735822	10405.217860	27.583808
251.017630	10417.644291	27.588826
251.300998	10435.686970	27.593844
251.653462	10448.289235	27.598861
251.970927	10464.297617	27.603879
252.544317	10480.447216	27.608896
252.425887	10499.486921	27.613914
252.790348	10508.596323	27.618932
253.013508	10533.297676	27.623949
253.413713	10543.460828	27.628967
253.722008	10552.145451	27.633984
253.761773	10566.219267	27.639002
254.131661	10565.994212	27.644020
254.185785	10593.418068	27.649037
254.736450	10595.023979	27.654055
255.024184	10619.067164	27.659072
255.058747	10631.131313	27.664090
255.577705	10646.633813	27.669108
255.620960	10664.676318	27.674125
255.802972	10671.145993	27.679143
256.312462	10686.319203	27.684160
256.155738	10695.399174	27.689178
256.636644	10716.383605	27.694196
256.685184	10737.748475	27.699213
257.071210	10752.015670	27.704231
257.470657	10758.556535	27.709248
257.383429	10785.208384	27.714266
257.904483	10794.834858	27.719284
257.715966	10807.244906	27.724301
258.258340	10833.080387	27.729319
258.704846	10841.408235	27.734336
258.620890	10867.569630	27.739354
258.978276	10889.973972	27.744372
259.371142	10907.768212	27.749389
259.365201	10922.480193	27.754407
259.779526	10932.179568	27.759424
260.042550	10955.378030	27.764442
260.448678	10968.401992	27.769460
260.573410	10996.720888	27.774477
260.700156	11014.329242	27.779495
261.067630	11020.815629	27.784512
261.275098	11043.938326	27.789530
261.663106	11057.453838	27.794548
261.803687	11079.153736	27.799565
261.974341	11087.365076	27.804583
262.100737	11103.270210	27.809600
262.333888	11122.588080	27.814618
262.596722	11139.698168	27.819636
262.795652	11164.908737	27.824653
263.135985	11186.195957	27.829671
263.540249	11192.482507	27.834688
263.807605	11227.957316	27.839706
264.183747	11234.886718	27.844724
264.355178	11251.019329	27.849741
264.522858	11276.027245	27.854759
265.057269	11286.674471	27.859776
265.256266	11309.393980	27.864794
265.877178	11318.563026	27.869812
265.784037	11331.189322	27.874829
266.165071	11351.935840	27.879847
266.621319	11365.643589	27.884864
266.615494	11384.968241	27.889882
266.828661	11393.881795	27.894900
267.114848	11416.312836	27.899917
267.473583	11426.806447	27.904935
267.882049	11449.244081	27.909952
268.178509	11474.145893	27.914970
268.240998	11475.180338	27.919988
268.474770	11494.528489	27.925005
268.814027	11515.389286	27.930023
269.147435	11532.986055	27.935040
269.333051	11555.243268	27.940058
269.703774	11568.007269	27.945076
269.578814	11587.509463	27.950093
269.801814	11593.818297	27.955111
270.506902	11621.333110	27.960128
270.557023	11640.150855	27.965146
271.070430	11658.556287	27.970164
271.257560	11679.957763	27.975181
271.395160	11694.219643	27.980199
271.921671	11712.722243	27.985216
272.193826	11734.724279	27.990234
272.429117	11746.833246	27.995252
272.810631	11755.068325	28.000269
272.939347	11780.080317	28.005287
273.185726	11786.560272	28.010304
273.775590	11816.964038	28.015322
273.843604	11830.057274	28.020340
274.006657	11840.228990	28.025357
274.259653	11864.933742	28.030375
274.813065	11877.161910	28.035392
274.965857	11894.743273	28.040410
275.350105	11909.856426	28.045428
275.517166	11927.362975	28.050445
275.802665	11947.349192	28.055463
275.942604	11956.796776	28.060480
275.937388	11980.465009	28.065498
276.538636	11996.506728	28.070516
276.637473	12020.673090	28.075533
276.808677	12050.576148	28.080551
277.067754	12062.883120	28.085568
277.353568	12090.217579	28.090586
277.910787	12094.937996	28.095604
278.144479	12123.685210	28.100621
278.370493	12141.883480	28.105639
278.953675	12153.074753	28.110656
279.027216	12168.491716	28.115674
279.273418	12182.754958	28.120692
279.661033	12199.007162	28.125709
280.091647	12219.054788	28.130727
280.514277	12229.654958	28.135744
280.924584	12241.054556	28.140762
280.985110	12247.625344	28.145780
281.348344	12253.424285	28.150797
281.381702	12265.089582	28.155815
281.943194	12266.547325	28.160832
281.792525	12284.612704	28.165850
281.599795	12304.642280	28.170868
282.223839	12315.543248	28.175885
282.215092	12345.200861	28.180903
282.760036	12354.978752	28.185920
282.943707	12376.217831	28.190938
283.140484	12397.229419	28.195956
283.512245	12412.619310	28.200973
283.395329	12434.921506	28.205991
284.225281	12461.184750	28.211008
284.005094	12483.552959	28.216026
284.405387	12507.105981	28.221044
284.952845	12533.195480	28.226061
285.140416	12559.859909	28.231079
285.441019	12576.620146	28.236096
285.876550	12597.540467	28.241114
285.743038	12620.406679	28.246132
286.641850	12640.032205	28.251149
286.378821	12662.826938	28.256167
287.153989	12668.061434	28.261184
287.321676	12700.758753	28.266202
287.779513	12716.936817	28.271220
288.327880	12730.654115	28.276237
288.404027	12755.855964	28.281255
288.517313	12764.685950	28.286272
288.718521	12788.251848	28.291290
289.403092	12800.693815	28.296308
289.585961	12818.851133	28.301325
289.684131	12841.966120	28.306343
290.308622	12864.206060	28.311360
290.472154	12881.179987	28.316378
290.291355	12899.397593	28.321396
291.055148	12917.744101	28.326413
291.314847	12937.601855	28.331431
291.943986	12946.745257	28.336448
291.877995	12972.320824	28.341466
291.971426	12984.105919	28.346484
292.431154	13005.738230	28.351501
292.706737	13020.526856	28.356519
293.261379	13050.458109	28.361536
293.379886	13068.780801	28.366554
293.100045	13089.421462	28.371572
294.045512	13106.091259	28.376589
293.703647	13136.115912	28.381607
294.475472	13149.021214	28.386624
294.766229	13175.299224	28.391642
295.002704	13195.559851	28.396660
295.062576	13212.385808	28.401677
295.568097	13245.252082	28.406695
295.729043	13253.221855	28.411712
296.132789	13276.058362	28.416730
296.350734	13300.455909	28.421748
296.882785	13316.274000	28.426765
297.253730	13336.939628	28.431783
297.907793	13352.245858	28.436800
298.185918	13371.495923	28.441818
298.213939	13385.987029	28.446836
298.857371	13399.690735	28.451853
298.490136	13418.979916	28.456871
298.905027	13427.333250	28.461888
299.121535	13450.402719	28.466906
299.584296	13471.143150	28.471924
300.323556	13488.898649	28.476941
299.966049	13507.967265	28.481959
300.035479	13528.831187	28.486976
300.279571	13542.829633	28.491994
301.011724	13556.356460	28.497012
301.236347	13575.593558	28.502029
301.260583	13594.064827	28.507047
301.419612	13618.196804	28.512064
301.809845	13643.970548	28.517082
302.087077	13668.735493	28.522100
302.456435	13691.025102	28.527117
302.571295	13716.001387	28.532135
302.770014	13733.949069	28.537152
302.836186	13757.196728	28.542170
303.524982	13792.856381	28.547188
303.700969	13811.250768	28.552205
304.022377	13850.172223	28.557223
304.252127	13865.000723	28.562240
304.791450	13899.051030	28.567258
305.015381	13928.126127	28.572276
305.828484	13931.723587	28.577293
305.888540	13969.188220	28.582311
306.588706	13987.161922	28.587328
306.997246	13998.785268	28.592346
307.050845	14029.753174	28.597364
307.885583	14032.669386	28.602381
307.342510	14061.840161	28.607399
307.917792	14080.848024	28.612416
308.677598	14094.507837	28.617434
308.438903	14130.186215	28.622452
308.715022	14140.851289	28.627469
309.145484	14165.238590	28.632487
309.496783	14191.451477	28.637504
309.891939	14222.886456	28.642522
310.118572	14230.319436	28.647540
310.659847	14258.248816	28.652557
310.308300	14272.883914	28.657575
310.495222	14294.834174	28.662592
311.067635	14324.273097	28.667610
311.419856	14359.630361	28.672628
312.055301	14375.139221	28.677645
312.252576	14401.998907	28.682663
312.756808	14422.533523	28.687680
313.101198	14447.255433	28.692698
312.945177	14467.642496	28.697716
313.638443	14495.958477	28.702733
313.532722	14523.138023	28.707751
313.743334	14546.871965	28.712768
314.521345	14565.553686	28.717786
314.550785	14590.830713	28.722804
315.084097	14605.467790	28.727821
315.352349	14635.893812	28.732839
315.559863	14653.629852	28.737856
316.158302	14685.965113	28.742874
316.378618	14705.536808	28.747892
316.643480	14722.265765	28.752909
316.855667	14758.624245	28.757927
317.293664	14771.308706	28.762944
317.832002	14794.148700	28.767962
317.959291	14817.392474	28.772980
318.420020	14829.641366	28.777997
318.362557	14850.264766	28.783015
318.798749	14877.344164	28.788032
319.640907	14905.185442	28.793050
319.592103	14920.191823	28.798068
319.927640	14944.621216	28.803085
320.139437	14969.446243	28.808103
320.395412	14998.213743	28.813120
320.832119	15007.918164	28.818138
321.120313	15043.103094	28.823156
321.421289	15051.580143	28.828173
321.637111	15076.535483	28.833191
322.124083	15094.053945	28.838208
322.602981	15112.316118	28.843226
322.436594	15130.677241	28.848244
323.036432	15151.034605	28.853261
323.217032	15177.956637	28.858279
323.445854	15200.140745	28.863296
324.007193	15215.300159	28.868314
323.881173	15243.855495	28.873332
324.744378	15263.633518	28.878349
325.003061	15292.459403	28.883367
325.193972	15308.072678	28.888384
325.422801	15324.823976	28.893402
325.333844	15350.539447	28.898420
325.950544	15368.991877	28.903437
326.723452	15402.997190	28.908455
326.711476	15424.939327	28.913472
327.196125	15451.430049	28.918490
327.806685	15469.297277	28.923508
328.138662	15493.559426	28.928525
328.603812	15510.807693	28.933543
328.584789	15537.520626	28.938560
329.130990	15549.301974	28.943578
329.655123	15576.164643	28.948596
330.007724	15598.078188	28.953613
330.128486	15611.432095	28.958631
329.963915	15648.901485	28.963648
330.928694	15657.710305	28.968666
330.879287	15696.136396	28.973684
331.139627	15715.921759	28.978701
331.420964	15742.047828	28.983719
331.539074	15762.774131	28.988736
331.889302	15788.609885	28.993754
332.110050	15832.306499	28.998772
332.621197	15848.366935	29.003789
332.943129	15877.805973	29.008807
333.043316	15903.339682	29.013824
334.131888	15926.883008	29.018842
333.891590	15970.366279	29.023860
334.061182	15977.748022	29.028877
334.512839	16013.231090	29.033895
334.675280	16047.253667	29.038912
335.287289	16072.866846	29.043930
335.736884	16116.907780	29.048948
336.581721	16130.288846	29.053965
336.876991	16155.595202	29.058983
337.074948	16180.832589	29.064000
337.498872	16204.546224	29.069018
338.175936	16232.984528	29.074036
338.054012	16242.547288	29.079053
338.574551	16264.203792	29.084071
338.898675	16291.937717	29.089088
339.081522	16300.477524	29.094106
339.664919	16327.638977	29.099124
339.738166	16350.572305	29.104141
340.460523	16382.562535	29.109159
340.413005	16403.436852	29.114176
340.741418	16419.569075	29.119194
341.038531	16453.749890	29.124212
341.305559	16475.242143	29.129229
341.645833	16495.119243	29.134247
341.580620	16519.812762	29.139264
342.188627	16541.311712	29.144282
342.507133	16573.738005	29.149300
342.801599	16605.708068	29.154317
343.049864	16625.140283	29.159335
343.441775	16656.351892	29.164352
343.926849	16683.393069	29.169370
344.221334	16708.473418	29.174388
344.944255	16726.708029	29.179405
345.098353	16752.475297	29.184423
345.279938	16778.105647	29.189440
345.718108	16787.453064	29.194458
345.979457	16818.360297	29.199476
346.025892	16845.040862	29.204493
347.085963	16862.724863	29.209511
347.082747	16891.352564	29.214528
347.472349	16913.783487	29.219546
347.994978	16932.798645	29.224564
348.285999	16964.257673	29.229581
348.611011	16980.457213	29.234599
348.871581	17012.074274	29.239616
349.124021	17025.833133	29.244634
349.497622	17061.339253	29.249652
349.489442	17083.757432	29.254669
350.184503	17103.366890	29.259687
350.375188	17139.327483	29.264704
350.899587	17162.381148	29.269722
350.962432	17199.966154	29.274740
351.532123	17224.010223	29.279757
352.012752	17260.060228	29.284775
352.014266	17297.327728	29.289792
352.679158	17314.924720	29.294810
352.754792	17344.630977	29.299828
352.994323	17376.040985	29.304845
353.554426	17405.205293	29.309863
353.874517	17443.247972	29.314880
354.423381	17465.334859	29.319898
354.775459	17496.428536	29.324916
355.204891	17526.238922	29.329933
355.375433	17540.678563	29.334951
356.082026	17578.939749	29.339968
356.580967	17594.289816	29.344986
356.834082	17626.524064	29.350004
356.929295	17653.550960	29.355021
357.689097	17664.212353	29.360039
358.070679	17699.154177	29.365056
358.659269	17724.780102	29.370074
358.805846	17743.442271	29.375092
359.047223	17769.675891	29.380109
359.167201	17790.798518	29.385127
359.391721	17825.968381	29.390144
360.097095	17844.547633	29.395162
360.442232	17880.908315	29.400180
360.668492	17903.384954	29.405197
361.172138	17932.704563	29.410215
361.128039	17960.686667	29.415232
361.561817	17985.854664	29.420250
362.099619	18018.515472	29.425268
362.214568	18047.738826	29.430285
363.258759	18068.248523	29.435303
363.224813	18095.376335	29.440320
363.511384	18114.460297	29.445338
364.232415	18140.799553	29.450356
364.305839	18177.056095	29.455373
365.007283	18187.092190	29.460391
365.187355	18225.270182	29.465408
365.482935	18249.711075	29.470426
365.865322	18271.646879	29.475444
366.133911	18298.661890	29.480461
366.610814	18321.423930	29.485479
366.931367	18354.337327	29.490496
366.714217	18375.458166	29.495514
367.540106	18406.774646	29.500532
367.819241	18443.842692	29.505549
368.297665	18461.593155	29.510567
368.564995	18484.454739	29.515584
368.740928	18511.825944	29.520602
369.061510	18542.148022	29.525620
369.245560	18570.793331	29.530637
369.954493	18603.367057	29.535655
369.773178	18634.697755	29.540672
370.449262	18655.089390	29.545690
370.917274	18696.450979	29.550708
370.793372	18721.750228	29.555725
371.332102	18749.857893	29.560743
371.689540	18788.219064	29.565760
371.980243	18827.573516	29.570778
372.592427	18858.089105	29.575796
373.019338	18898.658720	29.580813
373.465569	18924.650579	29.585831
373.732699	18957.090024	29.590848
374.220112	18998.613105	29.595866
374.754187	19025.169156	29.600884
374.756610	19066.495213	29.605901
375.485633	19088.147703	29.610919
375.517759	19119.281599	29.615936
376.265252	19155.911109	29.620954
376.661446	19192.415968	29.625972
377.045429	19218.681866	29.630989
377.309192	19248.248441	29.636007
377.482080	19273.862001	29.641024
377.866454	19305.286353	29.646042
378.619392	19343.583338	29.651060
378.965267	19382.881093	29.656077
379.249593	19411.798175	29.661095
379.565140	19446.109785	29.666112
379.764021	19478.334514	29.671130
380.572096	19513.269458	29.676148
380.667693	19552.355209	29.681165
381.602037	19577.710775	29.686183
381.454004	19612.733227	29.691200
382.131977	19651.257736	29.696218
382.410276	19671.907218	29.701236
382.873017	19714.284348	29.706253
383.036787	19747.973729	29.711271
383.746842	19779.100699	29.716288
383.859231	19806.161341	29.721306
384.496031	19835.701896	29.726324
384.902799	19865.480801	29.731341
385.329361	19905.513724	29.736359
385.302754	19925.031546	29.741376
385.693908	19957.072443	29.746394
386.316393	19991.864103	29.751412
386.741950	20034.863067	29.756429
387.166450	20059.982124	29.761447
387.549182	20096.007164	29.766464
387.824078	20125.820971	29.771482
388.506273	20151.602256	29.776500
388.795468	20180.833602	29.781517
389.344199	20204.582738	29.786535
389.082926	20243.645602	29.791552
389.494235	20285.088294	29.796570
390.363562	20313.050850	29.801588
390.398629	20352.831158	29.806605
391.152639	20380.011987	29.811623
391.688285	20411.780730	29.816640
391.448221	20443.777248	29.821658
392.161215	20473.702052	29.826676
392.379031	20502.496430	29.831693
393.192662	20536.297410	29.836711
393.638091	20558.479620	29.841728
393.823132	20593.335467	29.846746
394.188688	20607.338707	29.851764
394.434550	20632.931225	29.856781
394.569035	20657.350266	29.861799
395.075804	20688.011195	29.866816
395.524028	20733.756306	29.871834
396.117856	20752.614263	29.876852
396.405421	20793.440139	29.881869
396.565915	20815.825938	29.886887
396.902905	20855.073423	29.891904
397.324367	20892.664124	29.896922
398.002152	20918.319607	29.901940
398.521084	20958.358669	29.906957
398.708027	20989.226018	29.911975
399.129616	21019.603655	29.916992
399.791579	21049.440177	29.922010
400.037687	21080.742527	29.927028
400.328039	21112.086490	29.932045
400.829882	21143.373435	29.937063
401.198934	21180.691224	29.942080
401.116051	21216.160313	29.947098
401.735989	21239.410348	29.952116
402.189650	21292.278062	29.957133
402.386701	21322.690254	29.962151
402.865854	21355.463459	29.967168
402.886860	21400.743425	29.972186
403.235865	21444.327854	29.977204
403.911504	21473.432839	29.982221
404.680506	21515.528885	29.987239
405.165282	21556.404381	29.992256
405.487985	21601.515120	29.997274
406.028953	21628.170332	30.002292
406.432441	21657.413705	30.007309
406.691219	21696.846380	30.012327
407.019103	21732.037281	30.017344
407.568503	21770.359296	30.022362
408.102919	21799.764150	30.027380
408.369941	21856.098697	30.032397
409.059112	21882.783393	30.037415
409.826201	21915.677168	30.042432
410.198069	21950.039746	30.047450
410.702548	21971.949147	30.052468
410.501579	22010.957228	30.057485
411.157314	22046.627474	30.062503
411.382425	22069.362167	30.067520
411.904156	22106.666191	30.072538
412.590045	22132.596544	30.077556
412.855962	22181.672817	30.082573
413.196806	22198.524431	30.087591
413.767905	22226.684595	30.092608
413.732613	22261.433704	30.097626
414.492442	22292.263804	30.102644
414.802292	22327.651297	30.107661
415.345583	22371.117657	30.112679
415.769750	22402.290490	30.117696
416.301490	22436.430493	30.122714
416.816976	22471.080992	30.127732
416.874865	22500.895486	30.132749
417.244889	22533.605464	30.137767
417.906312	22563.575629	30.142784
417.814369	22599.504812	30.147802
418.706140	22630.752052	30.152820
419.048790	22663.255514	30.157837
419.154193	22699.027676	30.162855
419.901526	22724.551404	30.167872
420.154986	22762.812687	30.172890
420.695494	22789.761524	30.177908
421.010127	22829.739486	30.182925
421.061930	22862.548492	30.187943
421.608901	22891.527412	30.192960
421.949775	22934.238707	30.197978
422.713159	22960.860786	30.202996
422.931103	23001.987345	30.208013
423.067224	23039.620577	30.213031
423.711498	23067.978176	30.218048
424.022874	23113.539488	30.223066
424.920521	23142.167500	30.228084
425.401413	23181.834935	30.233101
425.658823	23210.291489	30.238119
426.130191	23240.114538	30.243136
426.293786	23273.982852	30.248154
427.132404	23294.466765	30.253172
427.379505	23332.000277	30.258189
427.732970	23360.925295	30.263207
428.008747	23398.138826	30.268224
428.200896	23435.550777	30.273242
428.832045	23475.200335	30.278260
429.542124	23518.580527	30.283277
429.476212	23552.760184	30.288295
430.184379	23592.014076	30.293312
430.653690	23637.591651	30.298330
430.973945	23671.639829	30.303348
431.513948	23714.424201	30.308365
431.585618	23752.760371	30.313383
432.379805	23793.323543	30.318400
432.439264	23830.832436	30.323418
432.949131	23863.854563	30.328436
433.224108	23905.970495	30.333453
433.834591	23947.728229	30.338471
434.606318	23989.430995	30.343488
434.806758	24040.652359	30.348506
435.166787	24078.667144	30.353524
435.980079	24113.632828	30.358541
436.009962	24165.765898	30.363559
436.843788	24199.659169	30.368576
437.179443	24250.010366	30.373594
437.584807	24288.355589	30.378612
437.880433	24331.626662	30.383629
438.634039	24374.137633	30.388647
439.244289	24406.216922	30.393664
439.374777	24447.777764	30.398682
439.646104	24484.098657	30.403700
440.261204	24524.491349	30.408717
440.607150	24568.208871	30.413735
441.395495	24602.675041	30.418752
442.132234	24647.122907	30.423770
442.981973	24665.900297	30.428788
443.085464	24702.202119	30.433805
443.412221	24728.834567	30.438823
443.948807	24760.406291	30.443840
444.290661	24798.993416	30.448858
444.623330	24825.937290	30.453876
445.163625	24857.647360	30.458893
445.505054	24900.237314	30.463911
446.000725	24934.064997	30.468928
446.302904	24972.384671	30.473946
446.439769	25013.239308	30.478964
447.535134	25046.662019	30.483981
447.498400	25085.668857	30.488999
448.029924	25113.271027	30.494016
448.329761	25161.375624	30.499034
448.647746	25199.238993	30.504052
449.369582	25232.449472	30.509069
449.349591	25282.354738	30.514087
450.062589	25314.743604	30.519104
450.116756	25362.362674	30.524122
450.635549	25404.634343	30.529140
451.079398	25437.282466	30.534157
451.494336	25496.645183	30.539175
452.180353	25525.834246	30.544192
452.544595	25570.948606	30.549210
453.040758	25609.814819	30.554228
453.646649	25643.471102	30.559245
453.829333	25681.695426	30.564263
453.779100	25725.818962	30.569280
454.541984	25768.606276	30.574298
455.083655	25812.502753	30.579316
456.002855	25863.377188	30.584333
456.158811	25905.836305	30.589351
456.347753	25944.009706	30.594368
456.981729	25993.767798	30.599386
457.337087	26033.506774	30.604404
457.859864	26084.636725	30.609421
458.211182	26128.742151	30.614439
458.722635	26170.991682	30.619456
459.269035	26218.131055	30.624474
459.816329	26265.194704	30.629492
460.440872	26300.028908	30.634509
460.765664	26348.066447	30.639527
461.735059	26383.812138	30.644544
462.429384	26425.085718	30.649562
462.719940	26462.852309	30.654580
463.445274	26491.500260	30.659597
463.745662	26531.309413	30.664615
464.091854	26560.035995	30.669632
464.430331	26601.570768	30.674650
464.883271	26638.560122	30.679668
465.592385	26680.295564	30.684685
465.343953	26728.495265	30.689703
466.582012	26768.159251	30.694720
466.890626	26807.175915	30.699738
467.522809	26840.861731	30.704756
467.809763	26877.869603	30.709773
468.246085	26919.120818	30.714791
468.520948	26954.477917	30.719808
468.824936	26993.640872	30.724826
469.744614	27037.042591	30.729844
470.337794	27079.189338	30.734861
470.437796	27122.887798	30.739879
470.878572	27157.243115	30.744896
471.358639	27204.607508	30.749914
471.609975	27247.180313	30.754932
472.478203	27289.149564	30.759949
472.948376	27331.380371	30.764967
473.378659	27378.289761	30.769984
473.925777	27426.495390	30.775002
474.168894	27463.470757	30.780020
474.924272	27492.216344	30.785037
475.001702	27545.351751	30.790055
475.658863	27583.104279	30.795072
476.139088	27625.939820	30.800090
476.439468	27674.426719	30.805108
477.172110	27717.662357	30.810125
477.597232	27761.384331	30.815143
478.153573	27806.024776	30.820160
478.527068	27851.115161	30.825178
478.727204	27893.944084	30.830196
479.379279	27935.591043	30.835213
479.910593	27985.564286	30.840231
480.430995	28025.069158	30.845248
481.035631	28061.105819	30.850266
481.041998	28109.267180	30.855284
481.658125	28142.917174	30.860301
481.933345	28202.378539	30.865319
482.693169	28241.541431	30.870336
483.097778	28280.892538	30.875354
483.419022	28323.355458	30.880372
484.068326	28367.313160	30.885389
484.354261	28409.267913	30.890407
484.652884	28451.334237	30.895424
485.506864	28501.738241	30.900442
485.573125	28545.442701	30.905460
486.464151	28586.382868	30.910477
486.439569	28644.046660	30.915495
486.678583	28688.549441	30.920512
487.021321	28742.881266	30.925530
487.612039	28789.177963	30.930548
488.260796	28849.652350	30.935565
488.658311	28908.562720	30.940583
489.346761	28958.440188	30.945600
489.518654	29011.804195	30.950618
490.234379	29069.100802	30.955636
491.113820	29121.401602	30.960653
491.444889	29182.084300	30.965671
492.121306	29221.925721	30.970688
492.970754	29271.108606	30.975706
493.136827	29325.947866	30.980724
493.918941	29365.456633	30.985741
494.410535	29416.560539	30.990759
495.063629	29459.160598	30.995776
495.807446	29499.499441	31.000794
496.093195	29556.793081	31.005812
496.796853	29593.744076	31.010829
496.845081	29638.732001	31.015847
497.403575	29678.937867	31.020864
497.909863	29722.657633	31.025882
498.608869	29784.568756	31.030900
498.512309	29827.281146	31.035917
499.340792	29874.080872	31.040935
499.726914	29924.250903	31.045952
500.460461	29981.143706	31.050970
500.769624	30029.503176	31.055988
501.670306	30070.486241	31.061005
501.907047	30120.388135	31.066023
502.167688	30166.039523	31.071040
502.853232	30226.323274	31.076058
502.959369	30278.503094	31.081076
503.862530	30323.420708	31.086093
504.487528	30385.797374	31.091111
504.755105	30438.206514	31.096128
505.843474	30485.233049	31.101146
505.981624	30538.774502	31.106164
506.297897	30582.452129	31.111181
506.842658	30628.654019	31.116199
507.439888	30678.463134	31.121216
508.135673	30722.627302	31.126234
508.710451	30770.982718	31.131252
509.268934	30814.784908	31.136269
509.681815	30876.870279	31.141287
510.176520	30925.734733	31.146304
510.808347	30969.812294	31.151322
511.464086	31020.335233	31.156340
511.811694	31059.544252	31.161357
512.318776	31106.766452	31.166375
512.761565	31152.317684	31.171392
513.149935	31190.182433	31.176410
513.545973	31253.669683	31.181428
514.552266	31294.250034	31.186445
515.020365	31335.664177	31.191463
515.114513	31393.718054	31.196480
515.853639	31431.080386	31.201498
516.303093	31481.891205	31.206516
516.592772	31533.451170	31.211533
517.342062	31581.953472	31.216551
517.634387	31617.679962	31.221568
517.955123	31664.861919	31.226586
518.578302	31713.618945	31.231604
519.027968	31763.001175	31.236621
519.682569	31803.953273	31.241639
519.865374	31848.195680	31.246656
520.710356	31898.778168	31.251674
520.884342	31949.831546	31.256692
521.525080	31998.693734	31.261709
522.226517	32053.566482	31.266727
522.379883	32099.903252	31.271744
523.211697	32148.241994	31.276762
523.480127	32211.239465	31.281780
524.511018	32259.078566	31.286797
524.733660	32318.572013	31.291815
525.534824	32371.491810	31.296832
526.179241	32409.373597	31.301850
526.809912	32457.219507	31.306868
527.366600	32498.564914	31.311885
527.357895	32555.194410	31.316903
527.955623	32606.927406	31.321920
528.352084	32654.490744	31.326938
528.998155	32713.700874	31.331956
529.623951	32759.039782	31.336973
530.362880	32814.864801	31.341991
530.709487	32877.394146	31.347008
531.294934	32921.859754	31.352026
531.462337	32986.583834	31.357044
532.192712	33037.800713	31.362061
532.859938	33086.080890	31.367079
533.106901	33149.025279	31.372096
534.136070	33201.486974	31.377114
534.113302	33261.683699	31.382132
534.551002	33310.725098	31.387149
535.274705	33371.114232	31.392167
535.594694	33429.553929	31.397184
536.560466	33491.301358	31.402202
537.173156	33548.711609	31.407220
537.897281	33602.086453	31.412237
539.036495	33652.663120	31.417255
539.460058	33707.479663	31.422272
539.684149	33737.639316	31.427290
540.045494	33796.095460	31.432308
540.339794	33856.071314	31.437325
541.308366	33898.434225	31.442343
541.588080	33959.892868	31.447360
542.339458	34009.730016	31.452378
542.813985	34062.153483	31.457396
543.215315	34112.787284	31.462413
543.820654	34165.230432	31.467431
544.217235	34226.582292	31.472448
544.773026	34274.177233	31.477466
545.512254	34337.972151	31.482484
546.305223	34390.201876	31.487501
546.665493	34439.281276	31.492519
547.093503	34489.151177	31.497536
547.839662	34544.058915	31.502554
547.963772	34602.635843	31.507572
548.640747	34652.073678	31.512589
549.346483	34703.337284	31.517607
549.627407	34773.537071	31.522624
550.368684	34822.592344	31.527642
550.754047	34873.470782	31.532660
551.121047	34936.508894	31.537677
551.978746	34987.899651	31.542695
551.861407	35045.757404	31.547712
552.776330	35103.330921	31.552730
553.363394	35155.865201	31.557748
553.671599	35206.962486	31.562765
554.494586	35261.253766	31.567783
554.825636	35316.428224	31.572800
555.666145	35370.076274	31.577818
556.234195	35433.051300	31.582836
556.859365	35471.671804	31.587853
557.479706	35531.201653	31.592871
557.651800	35583.913151	31.597888
558.649663	35633.054423	31.602906
559.248504	35690.798897	31.607924
559.174302	35743.400126	31.612941
560.037540	35795.739088	31.617959
560.302704	35858.996111	31.622976
561.300377	35916.283963	31.627994
561.715904	35980.974635	31.633012
562.382656	36039.277081	31.638029
562.877477	36086.785919	31.643047
563.244388	36148.565849	31.648064
563.918674	36199.621154	31.653082
564.426912	36260.061982	31.658100
565.057320	36328.524627	31.663117
565.762723	36384.722964	31.668135
566.116843	36452.783624	31.673152
566.628661	36505.574157	31.678170
567.493565	36570.000055	31.683188
567.702858	36636.554623	31.688205
568.329390	36689.487678	31.693223
568.871219	36763.325851	31.698240
569.534299	36818.607769	31.703258
570.132835	36888.229826	31.708276
570.487790	36947.688319	31.713293
571.580521	37008.934464	31.718311
571.707754	37072.887677	31.723328
572.645348	37131.142516	31.728346
573.401311	37205.117496	31.733364
573.647861	37259.204008	31.738381
574.550872	37322.868767	31.743399
574.972941	37380.101843	31.748416
575.985084	37435.113255	31.753434
576.591974	37486.521069	31.758452
577.368772	37549.421579	31.763469
577.912465	37594.584276	31.768487
578.277994	37651.319388	31.773504
578.573641	37703.776727	31.778522
579.357358	37762.444133	31.783540
580.088024	37822.515633	31.788557
580.894118	37873.033040	31.793575
581.280712	37938.474081	31.798592
581.857604	37988.837193	31.803610
582.708670	38045.578420	31.808628
582.831606	38090.477385	31.813645
583.967232	38142.983236	31.818663
584.418999	38205.785130	31.823680
584.932638	38258.466827	31.828698
585.614168	38307.001692	31.833716
585.849974	38361.888689	31.838733
586.534152	38419.690867	31.843751
586.806658	38473.656743	31.848768
587.288077	38521.445632	31.853786
587.779644	38585.678463	31.858804
588.626238	38651.481550	31.863821
589.278287	38702.339244	31.868839
589.635789	38770.799428	31.873856
590.306402	38829.511080	31.878874
590.658395	38892.890558	31.883892
591.094409	38955.767082	31.888909
591.769814	39014.424873	31.893927
592.062562	39074.512978	31.898944
592.493569	39130.910411	31.903962
593.594084	39196.105253	31.908980
593.488883	39259.365935	31.913997
594.707577	39324.282836	31.919015
594.837215	39384.468391	31.924032
595.760395	39443.345406	31.929050
596.415249	39503.589658	31.934068
596.929740	39569.754039	31.939085
597.587710	39640.475302	31.944103
598.003023	39701.006059	31.949120
598.460525	39770.855015	31.954138
599.031255	39835.609460	31.959156
599.933569	39896.076065	31.964173
600.496643	39966.362869	31.969191
600.942003	40029.513007	31.974208
601.667086	40102.194770	31.979226
602.522799	40167.250478	31.984244
602.950834	40227.076896	31.989261
603.577000	40307.967759	31.994279
604.031732	40371.164871	31.999296
604.327321	40446.656031	32.004314
605.222748	40513.287971	32.009332
605.664589	40602.740456	32.014349
606.325743	40652.544497	32.019367
607.136007	40737.886401	32.024384
607.475603	40813.075030	32.029402
608.866810	40865.123380	32.034420
608.895269	40948.142685	32.039437
609.629965	41008.075586	32.044455
610.132921	41086.827744	32.049472
610.605195	41159.138784	32.054490
611.873243	41231.997192	32.059508
611.945946	41296.277226	32.064525
612.765757	41366.400606	32.069543
613.766760	41428.424943	32.074560
614.050870	41497.832417	32.079578
614.902397	41569.813965	32.084596
615.076343	41639.821091	32.089613
615.752937	41713.789513	32.094631
616.757981	41777.396040	32.099648
616.986632	41851.360197	32.104666
617.870588	41925.086786	32.109684
618.546141	42002.570382	32.114701
619.188472	42061.306489	32.119719
619.893176	42124.695545	32.124736
620.407181	42203.232775	32.129754
620.895241	42277.263050	32.134772
621.401098	42340.483684	32.139789
622.219453	42415.770087	32.144807
623.182895	42487.777724	32.149824
623.453688	42552.600781	32.154842
624.508707	42620.530459	32.159860
624.810347	42691.878021	32.164877
625.618422	42745.821455	32.169895
626.424842	42816.833400	32.174912
626.753740	42890.709327	32.179930
627.343869	42957.899422	32.184948
627.790643	43030.866051	32.189965
628.680355	43097.246176	32.194983
628.965308	43165.740957	32.200000
629.685799	43239.026203	32.205018
630.588589	43313.917073	32.210036
631.129005	43386.080263	32.215053
631.578211	43450.741155	32.220071
632.239954	43522.212280	32.225088
632.701352	43596.874205	32.230106
633.648733	43665.485393	32.235124
634.189738	43729.576359	32.240141
634.768046	43794.889608	32.245159
635.109118	43855.307279	32.250176
635.441805	43921.394129	32.255194
636.490336	43985.840886	32.260212
636.859592	44063.860496	32.265229
637.771287	44117.645507	32.270247
638.310954	44194.181872	32.275264
638.790669	44264.792380	32.280282
639.555988	44334.364443	32.285300
639.672699	44419.645372	32.290317
640.684906	44490.228620	32.295335
641.422884	44570.851131	32.300352
641.787686	44640.443230	32.305370
642.559673	44721.370200	32.310388
642.963335	44800.066051	32.315405
644.062390	44873.452936	32.320423
644.688141	44961.310794	32.325440
644.767663	45034.488071	32.330458
646.087679	45123.400143	32.335476
646.355930	45203.979932	32.340493
647.009703	45286.504557	32.345511
647.746416	45365.892877	32.350528
648.487433	45451.400425	32.355546
649.034981	45529.333456	32.360564
649.532583	45618.001843	32.365581
650.182918	45689.760977	32.370599
651.014954	45780.702045	32.375616
651.252558	45859.903450	32.380634
652.690256	45942.389662	32.385652
653.024137	46024.645184	32.390669
653.639228	46109.677613	32.395687
654.452341	46180.369603	32.400704
655.085419	46273.190118	32.405722
656.010859	46342.623104	32.410740
656.568934	46434.559991	32.415757
657.074246	46519.265055	32.420775
657.957254	46591.740687	32.425792
658.698402	46666.728487	32.430810
659.257573	46743.903540	32.435828
659.713890	46818.875905	32.440845
660.329194	46907.625589	32.445863
661.108788	46988.368370	32.450880
661.643118	47077.599620	32.455898
662.496805	47157.108728	32.460916
662.883438	47239.136565	32.465933
663.726332	47323.650410	32.470951
664.601086	47407.568811	32.475968
664.988196	47501.361314	32.480986
665.998203	47581.768480	32.486004
666.388673	47643.118546	32.491021
667.340935	47731.364719	32.496039
667.985624	47809.076286	32.501056
668.598823	47892.910613	32.506074
669.457964	47974.452886	32.511092
669.667873	48051.833132	32.516109
670.581101	48145.020664	32.521127
671.532683	48215.299384	32.526144
671.825876	48300.559077	32.531162
672.682422	48376.301946	32.536180
673.416027	48459.149274	32.541197
673.839868	48539.559543	32.546215
674.874090	48626.880412	32.551232
675.050062	48707.379765	32.556250
676.053173	48776.897205	32.561268
676.887200	48866.317776	32.566285
677.295146	48937.390218	32.571303
677.800007	49018.247038	32.576320
678.438922	49102.376123	32.581338
679.680109	49167.174997	32.586356
679.958877	49246.958459	32.591373
681.008229	49319.416929	32.596391
681.548457	49387.184485	32.601408
681.943648	49469.602617	32.606426
682.619936	49539.849620	32.611444
683.189852	49617.839874	32.616461
683.719832	49699.226008	32.621479
684.338103	49781.873875	32.626496
684.657716	49864.903140	32.631514
685.618305	49955.744918	32.636532
686.271674	50046.663217	32.641549
687.171778	50130.608295	32.646567
688.032800	50208.979172	32.651584
688.416502	50298.913608	32.656602
689.324308	50381.768823	32.661620
690.071102	50475.794289	32.666637
690.550245	50560.325714	32.671655
691.646235	50643.668920	32.676672
691.801380	50727.919870	32.681690
692.586849	50810.405498	32.686708
693.479531	50905.653396	32.691725
693.823997	50998.099172	32.696743
694.362311	51087.556850	32.701760
694.956173	51189.975110	32.706778
695.818033	51277.383878	32.711796
696.638826	51376.941748	32.716813
696.997852	51469.899063	32.721831
697.669163	51565.388975	32.726848
698.745940	51670.560070	32.731866
699.909838	51766.304301	32.736884
700.381358	51858.916356	32.741901
700.807009	51953.185311	32.746919
701.994110	52040.998568	32.751936
702.044410	52143.960315	32.756954
703.089645	52226.244720	32.761972
703.955633	52325.711517	32.766989
704.849415	52423.714840	32.772007
706.115068	52508.566854	32.777024
706.565556	52601.072190	32.782042
707.200610	52682.598754	32.787060
708.043655	52772.057976	32.792077
708.808050	52856.678537	32.797095
709.429314	52937.671430	32.802112
709.918841	53044.330685	32.807130
710.698040	53124.938107	32.812148
711.420028	53211.746893	32.817165
711.693379	53310.078420	32.822183
713.072332	53390.568762	32.827200
713.614547	53485.426024	32.832218
713.939910	53570.886776	32.837236
714.994103	53661.964138	32.842253
715.534647	53753.922977	32.847271
716.383502	53854.973579	32.852288
716.816587	53945.093556	32.857306
717.758009	54043.842640	32.862324
718.512961	54124.603494	32.867341
718.905553	54227.279450	32.872359
719.759462	54319.100632	32.877376
720.619233	54406.207811	32.882394
720.989512	54506.374222	32.887412
721.762099	54600.446860	32.892429
722.304640	54704.300981	32.897447
723.456329	54800.573848	32.902464
723.764498	54897.719667	32.907482
724.704090	54991.305289	32.912500
725.213561	55070.227708	32.917517
725.783353	55171.539727	32.922535
726.467106	55255.899605	32.927552
726.983746	55351.174453	32.932570
727.832545	55443.766256	32.937588
728.852805	55545.915553	32.942605
729.639534	55645.829275	32.947623
730.064949	55726.828110	32.952640
730.709262	55828.725117	32.957658
731.813990	55920.227891	32.962676
732.620718	56005.227766	32.967693
733.345241	56109.962734	32.972711
734.285688	56190.499127	32.977728
734.812120	56290.825644	32.982746
735.692725	56378.664722	32.987764
736.395901	56479.436872	32.992781
736.987725	56572.720978	32.997799
737.744286	56654.711442	33.002816
738.437444	56767.315922	33.007834
739.388053	56862.431430	33.012852
740.230008	56963.739147	33.017869
740.709988	57043.893864	33.022887
741.437267	57148.994022	33.027904
742.151490	57248.112596	33.032922
742.879771	57350.584854	33.037940
743.790695	57452.256472	33.042957
744.455086	57556.794118	33.047975
745.432102	57651.169649	33.052992
746.385225	57748.785094	33.058010
746.758956	57846.547413	33.063028
747.805647	57941.494169	33.068045
748.417542	58046.371660	33.073063
749.087312	58142.790958	33.078080
749.955246	58238.109939	33.083098
750.764902	58338.027009	33.088116
751.378617	58430.564113	33.093133
752.034879	58533.705238	33.098151
753.013446	58637.969030	33.103168
753.957072	58735.641395	33.108186
754.690733	58837.892837	33.113204
755.789583	58936.804442	33.118221
756.379162	59031.048305	33.123239
756.936531	59127.200196	33.128256
757.810326	59216.108234	33.133274
758.525307	59317.240263	33.138292
759.315251	59412.520817	33.143309
760.111722	59516.326316	33.148327
760.857687	59603.822580	33.153344
761.452502	59708.092175	33.158362
761.784866	59808.727471	33.163380
763.023545	59904.745074	33.168397
763.771204	60003.302864	33.173415
764.587268	60106.109568	33.178432
765.579100	60205.285239	33.183450
766.076083	60313.909744	33.188468
766.866785	60402.179432	33.193485
767.537779	60502.313412	33.198503
768.644242	60606.477702	33.203520
769.639375	60695.410075	33.208538
770.058923	60798.443876	33.213556
770.889746	60890.305307	33.218573
771.490013	60994.220334	33.223591
772.112540	61086.982998	33.228608
773.034799	61195.598737	33.233626
773.846312	61288.090877	33.238644
774.648815	61385.755098	33.243661
775.316369	61490.995147	33.248679
776.032468	61585.918862	33.253696
776.824087	61675.761409	33.258714
777.299973	61776.869362	33.263732
777.982031	61866.395875	33.268749
778.582859	61968.703992	33.273767
779.434019	62062.962866	33.278784
780.270286	62162.344438	33.283802
781.012031	62275.116888	33.288820
781.884768	62373.204009	33.293837
782.668785	62479.093548	33.298855
783.417472	62577.044141	33.303872
784.185958	62676.060158	33.308890
784.394827	62796.761528	33.313908
785.722548	62884.934133	33.318925
785.917232	63001.517780	33.323943
786.798790	63120.542166	33.328960
787.736611	63223.167397	33.333978
788.303177	63341.910147	33.338996
789.196263	63450.694343	33.344013
789.956530	63568.932270	33.349031
790.854719	63679.284477	33.354048
791.885651	63791.043915	33.359066
792.317092	63912.821202	33.364084
793.337777	64029.394114	33.369101
794.503971	64147.087778	33.374119
795.393633	64250.389813	33.379136
796.163962	64359.995585	33.384154
796.597556	64484.936579	33.389172
797.412543	64589.649693	33.394189
798.233969	64715.672111	33.399207
799.301493	64824.580056	33.404224
800.316911	64941.519288	33.409242
800.890622	65051.913497	33.414260
801.939150	65160.010850	33.419277
802.473049	65280.622333	33.424295
803.392447	65384.892299	33.429312
804.492198	65484.733012	33.434330
804.963608	65615.661229	33.439348
806.107729	65724.984767	33.444365
806.905427	65831.635135	33.449383
807.241674	65938.406627	33.454400
808.200378	66062.423070	33.459418
809.102199	66175.285067	33.464436
810.088410	66299.273074	33.469453
810.931995	66418.088691	33.474471
811.402317	66519.795979	33.479488
812.221016	66634.058723	33.484506
812.975627	66748.079804	33.489524
813.735742	66873.461534	33.494541
814.471988	66994.504601	33.499559
815.339440	67110.342420	33.504576
816.500591	67226.966837	33.509594
817.289115	67348.243535	33.514612
818.081020	67469.526692	33.519629
818.805912	67591.472836	33.524647
819.626546	67703.667316	33.529664
820.465667	67820.683368	33.534682
821.354660	67942.686586	33.539700
822.311385	68043.739098	33.544717
822.810623	68177.593322	33.549735
823.288590	68303.807883	33.554752
824.558938	68413.124504	33.559770
825.201900	68538.838974	33.564788
826.339178	68651.877598	33.569805
827.127569	68771.354173	33.574823
827.864433	68882.436975	33.579840
828.544396	69012.801689	33.584858
829.658288	69134.730299	33.589876
830.617631	69243.426087	33.594893
831.271741	69355.972986	33.599911
831.599578	69463.731069	33.604928
833.050870	69568.028573	33.609946
833.585076	69684.510958	33.614964
834.295438	69790.316837	33.619981
835.114563	69907.651184	33.624999
835.822254	70021.678650	33.630016
836.823864	70140.059016	33.635034
837.664384	70245.175363	33.640052
838.313848	70360.807705	33.645069
839.049053	70495.788268	33.650087
839.827009	70610.679852	33.655104
841.112510	70730.717488	33.660122
841.658379	70856.961195	33.665140
842.317273	70969.863566	33.670157
843.354716	71094.073432	33.675175
844.251544	71236.765463	33.680192
844.849168	71355.396403	33.685210
845.753797	71477.954721	33.690228
846.328078	71602.497064	33.695245
847.501492	71728.610462	33.700263
848.483195	71869.104667	33.705280
849.472060	71977.297202	33.710298
850.199309	72116.089760	33.715316
851.486129	72241.150301	33.720333
852.315247	72368.152787	33.725351
852.797448	72493.872742	33.730368
853.573565	72608.459070	33.735386
854.543289	72748.265331	33.740404
855.222216	72874.467187	33.745421
856.463285	72991.875003	33.750439
857.378319	73141.058649	33.755456
858.094899	73249.631411	33.760474
858.715190	73394.868741	33.765492
860.015824	73524.095638	33.770509
861.041901	73644.571791	33.775527
861.634969	73777.901444	33.780544
862.594846	73906.921349	33.785562
863.188298	74024.302704	33.790580
864.316912	74151.063672	33.795597
865.666447	74283.632536	33.800615
866.201399	74400.133846	33.805632
867.457283	74517.174279	33.810650
868.245798	74651.374989	33.815668
869.462879	74771.971220	33.820685
870.324809	74899.868437	33.825703
870.631391	75031.488549	33.830720
871.929017	75143.642852	33.835738
872.388864	75273.063396	33.840756
873.240726	75393.495752	33.845773
874.270776	75512.735549	33.850791
875.028925	75646.068210	33.855808
875.928381	75761.687900	33.860826
876.799413	75891.550046	33.865844
877.499595	76019.986495	33.870861
878.255746	76147.402451	33.875879
879.021222	76283.761041	33.880896
880.385378	76403.987675	33.885914
881.183392	76543.125461	33.890932
882.197075	76664.980076	33.895949
883.281318	76787.101992	33.900967
883.643077	76920.387703	33.905984
884.788107	77040.932335	33.911002
885.794196	77181.058048	33.916020
886.173306	77302.964183	33.921037
887.185318	77434.450268	33.926055
887.795055	77552.783809	33.931072
888.883329	77688.724432	33.936090
889.793605	77808.742762	33.941108
890.420302	77937.600934	33.946125
891.847978	78060.742023	33.951143
892.487458	78190.750766	33.956160
893.212906	78297.841413	33.961178
893.621801	78427.516460	33.966196
894.179073	78553.935351	33.971213
895.141596	78688.239216	33.976231
896.334917	78831.228778	33.981248
896.880197	78959.973449	33.986266
897.825712	79104.852833	33.991284
898.411161	79243.074739	33.996301
899.765012	79377.096595	34.001319
900.358761	79523.422196	34.006336
901.509291	79658.896341	34.011354
902.744989	79810.810928	34.016372
903.343975	79951.622233	34.021389
904.307761	80087.306958	34.026407
905.182573	80242.940558	34.031424
906.240804	80377.010909	34.036442
907.005609	80512.851285	34.041460
908.069437	80661.213092	34.046477
909.150183	80807.985195	34.051495
909.929732	80955.794950	34.056512
910.872275	81096.575518	34.061530
912.015496	81241.163843	34.066548
912.517991	81387.725325	34.071565
913.679235	81535.146742	34.076583
914.372471	81679.508596	34.081600
915.244285	81816.224748	34.086618
916.088028	81971.286935	34.091636
917.415028	82127.326787	34.096653
918.319960	82269.329176	34.101671
918.863180	82426.481310	34.106688
919.918246	82578.475865	34.111706
921.047968	82730.326218	34.116724
921.725854	82879.734244	34.121741
923.119182	83028.607351	34.126759
924.279059	83178.386808	34.131776
924.742190	83327.137297	34.136794
925.741298	83478.096782	34.141812
926.582513	83626.027437	34.146829
927.624615	83770.028375	34.151847
928.397805	83928.108092	34.156864
929.254990	84078.784943	34.161882
930.254630	84228.825483	34.166900
931.199146	84382.438312	34.171917
932.613499	84530.355885	34.176935
933.111713	84678.071581	34.181952
934.222271	84831.229664	34.186970
935.151309	84976.446321	34.191988
936.328875	85136.745232	34.197005
937.281994	85279.466805	34.202023
938.113889	85426.878967	34.207040
939.277730	85579.805368	34.212058
940.199125	85723.351148	34.217076
940.960053	85880.243913	34.222093
942.098133	86021.117081	34.227111
943.072451	86182.734957	34.232128
944.080630	86316.455807	34.237146
945.373712	86459.685194	34.242164
945.937641	86617.355812	34.247181
946.875974	86761.582217	34.252199
947.833333	86911.286289	34.257216
948.754931	87058.130685	34.262234
949.610829	87196.039151	34.267252
950.123885	87348.926495	34.272269
950.825063	87492.905503	34.277287
951.955361	87648.249228	34.282304
952.981408	87783.835899	34.287322
953.983423	87935.171723	34.292340
955.035538	88080.963073	34.297357
955.888002	88211.309524	34.302375
956.618948	88363.275101	34.307392
957.778932	88504.317680	34.312410
958.710546	88651.309519	34.317428
959.357870	88804.829529	34.322445
960.876931	88941.144980	34.327463
961.663466	89098.352305	34.332480
962.142522	89241.283816	34.337498
962.841574	89399.792273	34.342516
963.961417	89547.878657	34.347533
965.440708	89709.582637	34.352551
966.377148	89874.978482	34.357568
966.946216	90032.208915	34.362586
967.919000	90181.981654	34.367604
968.686755	90347.509908	34.372621
969.921190	90507.797810	34.377639
971.178389	90670.956319	34.382656
971.759763	90837.138988	34.387674
973.056290	90994.426288	34.392692
973.412289	91160.863637	34.397709
974.850323	91322.711863	34.402727
975.869570	91487.275980	34.407744
976.601009	91663.015400	34.412762
977.827431	91819.357630	34.417780
978.802572	91997.806032	34.422797
980.029981	92152.359077	34.427815
980.757506	92331.097713	34.432832
982.102273	92486.981618	34.437850
983.013839	92655.369054	34.442868
983.728665	92831.252577	34.447885
984.881762	92993.791996	34.452903
986.147940	93155.320064	34.457920
987.115490	93316.904910	34.462938
988.067124	93473.201916	34.467956
989.043870	93654.934565	34.472973
989.951437	93822.957247	34.477991
991.224315	93985.780935	34.483008
992.110553	94145.985816	34.488026
993.118034	94311.571015	34.493044
993.989672	94489.826830	34.498061
995.250984	94646.023112	34.503079
996.212858	94814.296771	34.508096
997.117162	94986.771541	34.513114
998.056016	95138.966743	34.518132
999.205620	95314.264399	34.523149
1000.144450	95475.893470	34.528167
1001.274064	95652.488163	34.533184
1002.708791	95819.753595	34.538202
1003.783223	95968.171330	34.543220
1004.600803	96140.263320	34.548237
1005.661361	96296.737415	34.553255
1006.549540	96448.607178	34.558272
1007.318487	96617.779549	34.563290
1008.515786	96777.272633	34.568308
1008.940138	96950.118910	34.573325
1010.199258	97120.891204	34.578343
1011.362333	97283.457142	34.583360
1012.219566	97452.930749	34.588378
1013.572785	97621.690420	34.593396
1014.311830	97793.743448	34.598413
1015.347654	97958.943040	34.603431
1016.518066	98127.850285	34.608448
1017.329224	98286.378551	34.613466
1018.405726	98443.205252	34.618484
1019.698861	98612.823495	34.623501
1020.448642	98767.617037	34.628519
1021.546189	98912.794253	34.633536
1022.455667	99081.681372	34.638554
1023.743020	99216.104207	34.643572
1024.398626	99381.186020	34.648589
1025.685276	99530.729275	34.653607
1026.522782	99692.623799	34.658624
1027.243390	99852.151817	34.663642
1028.428886	100015.504007	34.668660
1029.242619	100179.532848	34.673677
1030.623323	100355.865728	34.678695
1031.593245	100513.989085	34.683712
1032.270233	100676.714135	34.688730
1033.419160	100845.510017	34.693748
1034.339404	101018.403307	34.698765
1035.612561	101193.328811	34.703783
1036.299105	101358.842474	34.708800
1037.379660	101540.285715	34.713818
1038.266309	101712.809324	34.718836
1039.330965	101889.502571	34.723853
1040.602876	102078.408360	34.728871
1041.599808	102248.302293	34.733888
1042.442398	102439.998046	34.738906
1043.862383	102611.844266	34.743924
1044.625323	102794.678511	34.748941
1045.768812	102966.971709	34.753959
1047.082938	103143.473948	34.758976
1048.098599	103341.903985	34.763994
1049.027343	103513.527113	34.769012
1050.132561	103697.355888	34.774029
1051.064973	103871.779569	34.779047
1052.375609	104050.435124	34.784064
1053.185281	104238.065241	34.789082
1054.465709	104414.891914	34.794100
1055.641814	104606.757387	34.799117
1056.490550	104783.657918	34.804135
1057.645332	104968.728551	34.809152
1058.515685	105158.596883	34.814170
1059.852996	105337.510067	34.819188
1060.789058	105523.178012	34.824205
1062.004492	105710.219576	34.829223
1063.520670	105893.121826	34.834240
1064.364172	106077.061138	34.839258
1065.492872	106252.911963	34.844276
1066.796515	106442.439206	34.849293
1067.577569	106618.869219	34.854311
1069.137298	106796.653546	34.859328
1069.950248	106976.576403	34.864346
1071.275500	107154.591870	34.869364
1072.153247	107330.820607	34.874381
1073.425058	107503.071520	34.879399
1074.812599	107682.422802	34.884416
1075.397103	107866.113262	34.889434
1076.486516	108030.088636	34.894452
1077.657174	108215.001862	34.899469
1078.401633	108400.620151	34.904487
1079.801188	108572.185461	34.909504
1080.941778	108759.552045	34.914522
1081.920210	108924.539206	34.919540
1082.810609	109110.087566	34.924557
1084.069044	109296.969708	34.929575
1085.107966	109465.129560	34.934592
1086.337969	109659.353105	34.939610
1087.606708	109835.964221	34.944628
1088.429579	110017.299092	34.949645
1089.172372	110199.915144	34.954663
1090.485323	110370.606751	34.959680
1091.201950	110541.398018	34.964698
1092.332000	110709.664480	34.969716
1093.240434	110889.078174	34.974733
1094.063604	111069.368545	34.979751
1095.407693	111236.576760	34.984768
1096.519776	111416.314924	34.989786
1097.771585	111594.409653	34.994804
1098.795268	111773.455353	34.999821
1099.474474	111955.054797	35.004839
1100.706332	112138.793674	35.009856
1101.476379	112327.056712	35.014874
1102.668046	112521.509524	35.019892
1103.858594	112712.378691	35.024909
1104.803116	112903.555887	35.029927
1106.213925	113085.877898	35.034944
1106.650499	113292.838256	35.039962
1108.098139	113487.800254	35.044980
1109.294802	113690.165774	35.049997
1110.517836	113884.432872	35.055015
1111.680210	114073.250948	35.060032
1112.633732	114284.960109	35.065050
1113.839779	114475.572700	35.070068
1114.899226	114683.061130	35.075085
1115.758850	114887.720817	35.080103
1117.218902	115089.761468	35.085120
1118.021338	115291.012740	35.090138
1119.104983	115494.132085	35.095156
1120.346718	115701.420474	35.100173
1121.173755	115912.111138	35.105191
1122.438878	116119.043947	35.110208
1123.937944	116330.817589	35.115226
1125.253626	116541.077353	35.120244
1126.504711	116751.767467	35.125261
1127.585405	116958.812880	35.130279
1128.948030	117148.454577	35.135296
1129.770608	117361.006557	35.140314
1131.295102	117563.244155	35.145332
1132.194662	117776.939514	35.150349
1133.416308	117972.881997	35.155367
1134.517692	118182.593684	35.160384
1135.225188	118393.398368	35.165402
1136.633471	118610.474986	35.170420
1138.067485	118815.942118	35.175437
1139.115899	119030.635827	35.180455
1140.222685	119237.845330	35.185472
1141.319987	119448.846658	35.190490
1142.465285	119657.738090	35.195508
1143.702353	119875.131224	35.200525
1144.644509	120088.912583	35.205543
1145.954843	120287.745172	35.210560
1146.976219	120514.454524	35.215578
1148.258732	120713.193217	35.220596
1149.664520	120925.978958	35.225613
1150.803040	121138.582320	35.230631
1151.796713	121344.659563	35.235648
1152.953278	121561.318128	35.240666
1153.978750	121782.701455	35.245684
1155.080242	121980.135309	35.250701
1156.219386	122196.674669	35.255719
1157.020542	122419.709256	35.260736
1158.264621	122628.998247	35.265754
1159.524200	122859.589408	35.270772
1161.338008	123073.412962	35.275789
1162.054963	123287.672839	35.280807
1163.462640	123503.176091	35.285824
1164.641327	123722.888275	35.290842
1165.709291	123930.327140	35.295860
1167.097807	124127.575629	35.300877
1167.876335	124346.560081	35.305895
1169.017087	124539.796669	35.310912
1170.455871	124738.358895	35.315930
1171.553701	124924.685159	35.320948
1172.604775	125129.549572	35.325965
1173.443558	125349.241038	35.330983
1174.866402	125544.579293	35.336000
1175.825951	125753.430025	35.341018
1176.614324	125960.624803	35.346036
1178.379550	126167.329960	35.351053
1179.154202	126400.791264	35.356071
1180.220079	126602.570533	35.361088
1181.335099	126821.783286	35.366106
1182.575861	127048.454895	35.371124
1183.560839	127274.549387	35.376141
1184.523154	127492.942936	35.381159
1185.968857	127721.296709	35.386176
1186.809097	127954.074460	35.391194
1187.929837	128193.588807	35.396212
1189.434240	128420.847948	35.401229
1190.497824	128654.468605	35.406247
1191.819931	128891.787533	35.411264
1193.135672	129121.275813	35.416282
1194.308530	129362.552404	35.421300
1195.798602	129586.666137	35.426317
1197.034958	129825.261196	35.431335
1198.461531	130060.961852	35.436352
1199.011068	130291.320526	35.441370
1200.540675	130528.237206	35.446388
1201.664728	130765.869186	35.451405
1202.589944	130993.876459	35.456423
1204.163261	131234.847603	35.461440
1205.338428	131477.661097	35.466458
1206.698064	131709.531388	35.471476
1208.153297	131937.508488	35.476493
1209.490487	132190.746199	35.481511
1210.635918	132424.267019	35.486528
1212.199744	132658.240123	35.491546
1213.508336	132883.193019	35.496564
1214.947869	133110.420398	35.501581
1215.828553	133348.808985	35.506599
1216.915958	133566.868743	35.511616
1218.456816	133795.935066	35.516634
1219.506161	134024.336278	35.521652
1221.073641	134256.367974	35.526669
1222.110563	134491.341501	35.531687
1223.354719	134711.563561	35.536704
1224.878887	134950.047643	35.541722
1225.309403	135182.806314	35.546740
1227.587840	135402.709900	35.551757
1228.469906	135636.157811	35.556775
1229.663830	135864.826845	35.561792
1231.014322	136097.655416	35.566810
1232.139787	136328.621061	35.571828
1233.561409	136554.531355	35.576845
1234.396324	136785.231236	35.581863
1235.886978	137010.131600	35.586880
1237.104913	137250.838233	35.591898
1238.208775	137472.065412	35.596916
1239.775545	137709.091528	35.601933
1240.800132	137936.877193	35.606951
1241.882497	138166.556710	35.611968
1243.250771	138392.767153	35.616986
1243.892307	138623.549658	35.622004
1245.511218	138861.462798	35.627021
1246.721636	139101.321686	35.632039
1248.292431	139327.974030	35.637056
1249.768037	139562.403535	35.642074
1250.520921	139779.303986	35.647092
1251.599024	139999.017680	35.652109
1253.023750	140211.042217	35.657127
1254.130012	140440.783846	35.662144
1255.262333	140663.891053	35.667162
1256.772091	140877.833008	35.672180
1258.306515	141092.076535	35.677197
1258.633945	141332.528104	35.682215
1260.036593	141554.024020	35.687232
1261.416562	141784.452115	35.692250
1262.363674	142023.246338	35.697268
1263.738766	142253.310606	35.702285
1264.709382	142497.062296	35.707303
1265.672463	142736.505466	35.712320
1267.091107	142982.684587	35.717338
1268.020529	143244.810165	35.722356
1269.195166	143491.083896	35.727373
1270.891066	143753.682568	35.732391
1272.368711	144002.636221	35.737408
1273.586331	144249.998712	35.742426
1274.715111	144510.261913	35.747444
1275.904284	144760.853732	35.752461
1276.963892	145025.989139	35.757479
1278.434899	145274.978139	35.762496
1279.911008	145528.787094	35.767514
1281.042368	145800.396743	35.772532
1282.413872	146056.002165	35.777549
1283.836744	146321.239256	35.782567
1284.984095	146589.466086	35.787584
1286.236309	146851.628140	35.792602
1287.407908	147118.637370	35.797620
1288.823127	147381.816246	35.802637
1289.987195	147653.764090	35.807655
1291.524839	147921.238659	35.812672
1292.947372	148189.939057	35.817690
1293.963463	148469.336769	35.822708
1295.584419	148731.096194	35.827725
1296.628013	149003.061226	35.832743
1297.886617	149279.710811	35.837760
1299.163879	149553.886152	35.842778
1300.466614	149833.170649	35.847796
1302.028861	150097.828491	35.852813
1303.437901	150381.031337	35.857831
1304.500811	150658.915711	35.862848
1305.785914	150931.983681	35.867866
1307.295279	151221.923950	35.872884
1308.971914	151485.240839	35.877901
1310.132824	151761.430163	35.882919
1311.500102	152025.715167	35.887936
1312.850106	152299.568649	35.892954
1313.799514	152580.403174	35.897972
1315.535256	152845.673040	35.902989
1317.045452	153122.867248	35.908007
1318.173477	153397.665833	35.913024
1319.631537	153658.243205	35.918042
1320.601706	153945.363071	35.923060
1321.783067	154215.693650	35.928077
1323.683482	154495.281321	35.933095
1324.841125	154765.847957	35.938112
1326.088360	155038.025328	35.943130
1327.438765	155322.327136	35.948148
1328.779507	155601.292142	35.953165
1330.382402	155873.746316	35.958183
1331.812118	156150.873818	35.963200
1333.277890	156410.098174	35.968218
1334.351147	156696.434574	35.973236
1335.615084	156956.850223	35.978253
1336.773966	157224.325474	35.983271
1337.948100	157480.433552	35.988288
1339.655243	157732.928505	35.993306
1340.758793	157992.159530	35.998324
1342.199463	158249.395540	36.003341
1343.547898	158505.189528	36.008359
1344.869688	158771.252627	36.013376
1346.260313	159028.146623	36.018394
1347.170386	159295.600553	36.023412
1348.464687	159554.365973	36.028429
1350.011788	159820.918798	36.033447
1350.779177	160098.956687	36.038464
1352.187346	160366.791969	36.043482
1353.626778	160654.998706	36.048500
1354.708116	160929.095446	36.053517
1355.981719	161212.499772	36.058535
1357.305350	161501.416592	36.063552
1358.914882	161785.670055	36.068570
1359.879528	162074.523276	36.073588
1361.670839	162368.989176	36.078605
1363.057241	162655.429523	36.083623
1364.241620	162951.864821	36.088640
1365.516649	163240.230629	36.093658
1366.771234	163541.352801	36.098676
1368.617856	163836.339903	36.103693
1370.080322	164130.796195	36.108711
1371.110093	164418.309623	36.113728
1372.692967	164714.589737	36.118746
1373.679949	165023.341191	36.123764
1375.134699	165319.405532	36.128781
1376.751299	165628.526676	36.133799
1377.929688	165927.711356	36.138816
1380.031523	166223.611426	36.143834
1381.203770	166533.028074	36.148852
1382.777249	166831.341528	36.153869
1384.454665	167123.574640	36.158887
1385.440245	167427.432681	36.163904
1387.141740	167720.109829	36.168922
1388.760787	168029.145811	36.173940
1390.129164	168320.042034	36.178957
1391.578320	168619.859882	36.183975
1392.764924	168913.340466	36.188992
1394.163844	169212.015819	36.194010
1395.525045	169506.956017	36.199028
1396.841596	169804.722542	36.204045
1398.717464	170103.794407	36.209063
1399.831341	170410.493675	36.214080
1401.736566	170707.090140	36.219098
1402.941689	171003.702685	36.224116
1404.687400	171294.669651	36.229133
1406.196193	171580.855432	36.234151
1407.172370	171880.924967	36.239168
1408.938361	172166.234278	36.244186
1410.126628	172470.561755	36.249204
1411.831050	172770.097827	36.254221
1412.999937	173057.338580	36.259239
1414.297711	173356.564840	36.264256
1416.057975	173644.536272	36.269274
1417.129214	173948.067651	36.274292
1418.269927	174242.947170	36.279309
1419.855220	174535.559534	36.284327
1421.184224	174840.284916	36.289344
1422.757606	175141.228028	36.294362
1424.304170	175435.375105	36.299380
1425.503135	175743.427247	36.304397
1426.858480	176030.426397	36.309415
1428.428625	176328.534529	36.314432
1430.037407	176635.839196	36.319450
1431.443009	176933.597420	36.324468
1432.586011	177211.246941	36.329485
1434.094496	177493.127306	36.334503
1435.385006	177778.865415	36.339520
1436.669959	178062.994232	36.344538
1437.958092	178355.665594	36.349556
1439.221914	178644.078243	36.354573
1440.924138	178939.235567	36.359591
1442.095722	179232.451586	36.364608
1443.369885	179528.241482	36.369626
1444.721397	179836.141159	36.374644
1446.173646	180138.479582	36.379661
1447.863151	180452.228884	36.384679
1448.773515	180759.001176	36.389696
1450.219198	181062.551803	36.394714
1451.846311	181375.415795	36.399732
1453.310147	181691.177118	36.404749
1455.081539	182002.523268	36.409767
1456.535251	182325.918251	36.414784
1458.065303	182640.861941	36.419802
1459.300676	182951.959498	36.424820
1460.637032	183274.859190	36.429837
1462.226295	183594.812340	36.434855
1463.485838	183925.255491	36.439872
1464.933545	184242.811479	36.444890
1466.557000	184561.596886	36.449908
1467.617906	184892.814894	36.454925
1469.338141	185221.971167	36.459943
1471.000961	185553.702938	36.464960
1473.009425	185881.571535	36.469978
1474.479485	186219.914308	36.474996
1475.628026	186549.769461	36.480013
1477.606860	186861.972092	36.485031
1478.905839	187197.759478	36.490048
1480.306658	187535.550325	36.495066
1482.069032	187855.562767	36.500084
1483.367752	188192.409609	36.505101
1485.030643	188513.711531	36.510119
1486.571137	188840.963592	36.515136
1487.882113	189166.059322	36.520154
1489.827090	189496.129781	36.525172
1491.276241	189828.073914	36.530189
1493.185310	190146.729069	36.535207
1494.467650	190484.353426	36.540224
1495.815622	190807.700212	36.545242
1497.457555	191134.808536	36.550260
1498.665927	191450.171557	36.555277
1500.536223	191781.650682	36.560295
1501.776005	192111.979009	36.565312
1503.360351	192436.209432	36.570330
1504.862631	192766.066274	36.575348
1506.205861	193102.704885	36.580365
1507.765966	193429.585070	36.585383
1509.311528	193772.376351	36.590400
1510.949239	194096.631994	36.595418
1512.499356	194431.529701	36.600436
1513.222540	194768.051162	36.605453
1515.110209	195107.352702	36.610471
1516.682395	195442.417101	36.615488
1518.193296	195772.821415	36.620506
1519.597641	196119.749275	36.625524
1521.000613	196466.971206	36.630541
1522.840082	196796.069540	36.635559
1524.276676	197137.512903	36.640576
1525.799028	197479.121595	36.645594
1526.914513	197815.098798	36.650612
1528.507059	198169.255671	36.655629
1529.991540	198507.638382	36.660647
1531.531103	198847.753044	36.665664
1533.405236	199174.800552	36.670682
1534.731675	199497.255206	36.675700
1535.979113	199829.208544	36.680717
1537.411669	200149.515728	36.685735
1538.857681	200480.702976	36.690752
1540.247937	200810.618656	36.695770
1541.503397	201155.628923	36.700788
1543.114067	201489.980527	36.705805
1544.382330	201828.783310	36.710823
1545.882200	202193.691940	36.715840
1547.936520	202540.176665	36.720858
1549.497356	202887.049301	36.725876
1550.805642	203234.714425	36.730893
1552.787062	203588.123264	36.735911
1553.767482	203938.385258	36.740928
1555.068188	204291.846426	36.745946
1556.919230	204659.058199	36.750964
1558.110552	205024.628545	36.755981
1559.564754	205395.337690	36.760999
1561.027157	205758.873290	36.766016
1562.802242	206126.587165	36.771034
1564.804651	206494.100154	36.776052
1566.081268	206872.921277	36.781069
1567.714405	207252.294797	36.786087
1569.126618	207624.799127	36.791104
1570.856518	208005.709353	36.796122
1572.462891	208383.086422	36.801140
1573.971199	208765.484376	36.806157
1576.067195	209147.380688	36.811175
1577.794772	209533.187105	36.816192
1579.218358	209911.426756	36.821210
1580.839816	210277.318338	36.826228
1582.310120	210675.667378	36.831245
1584.015871	211041.065802	36.836263
1585.919207	211423.829662	36.841280
1587.352098	211799.003199	36.846298
1588.956672	212176.461077	36.851316
1590.648664	212569.728289	36.856333
1592.300551	212940.324503	36.861351
1593.859797	213333.591625	36.866368
1595.135762	213717.586548	36.871386
1597.094986	214092.174851	36.876404
1598.766629	214489.796715	36.881421
1600.324103	214859.933805	36.886439
1602.167968	215248.844568	36.891456
1603.649248	215632.407159	36.896474
1605.468601	216001.337185	36.901492
1606.882731	216392.558624	36.906509
1608.589696	216770.373988	36.911527
1610.372267	217170.833311	36.916544
1612.058584	217549.645611	36.921562
1613.650516	217932.716441	36.926580
1615.005191	218321.136167	36.931597
1616.945930	218706.971520	36.936615
1618.529480	219095.889756	36.941632
1620.483066	219474.284120	36.946650
1621.850969	219853.970353	36.951668
1623.373818	220225.911143	36.956685
1625.415593	220614.505325	36.961703
1626.611179	220992.319177	36.966720
1628.072004	221377.303841	36.971738
1629.616881	221757.780332	36.976756
1631.204456	222151.204655	36.981773
1632.867513	222544.643290	36.986791
1634.599024	222922.933970	36.991808
1635.995028	223314.463636	36.996826
1638.050720	223711.321140	37.001844
1639.446223	224095.817851	37.006861
1640.936159	224470.927726	37.011879
1642.127795	224904.558331	37.016896
1643.713192	225276.657772	37.021914
1645.529158	225647.450258	37.026932
1647.505602	226028.783746	37.031949
1648.799476	226404.414537	37.036967
1650.381157	226793.105377	37.041984
1651.602867	227171.061762	37.047002
1653.555972	227549.939832	37.052020
1654.937838	227952.205516	37.057037
1656.972504	228335.466630	37.062055
1658.608845	228725.652780	37.067072
1659.670670	229119.948249	37.072090
1661.728246	229516.874419	37.077108
1663.319866	229923.353167	37.082125
1664.810344	230321.061099	37.087143
1666.841948	230728.536280	37.092160
1667.840592	231131.433258	37.097178
1669.428184	231534.767457	37.102196
1671.022291	231960.657833	37.107213
1672.970458	232372.342453	37.112231
1674.539881	232795.749896	37.117248
1675.831255	233222.785989	37.122266
1677.985251	233644.473434	37.127284
1679.554847	234072.075434	37.132301
1681.024155	234502.235251	37.137319
1683.404401	234928.994278	37.142336
1684.582297	235364.437126	37.147354
1686.637368	235779.389397	37.152372
1688.405167	236219.868039	37.157389
1689.930523	236650.506491	37.162407
1691.672435	237079.636858	37.167424
1693.349570	237515.434201	37.172442
1695.202574	237940.026603	37.177460
1696.939508	238381.429835	37.182477
1698.426210	238829.352901	37.187495
1700.343205	239259.398956	37.192512
1701.647762	239703.975502	37.197530
1703.701074	240129.987246	37.202548
1705.271597	240575.182089	37.207565
1706.775419	241025.418490	37.212583
1709.211456	241477.127526	37.217600
1710.641375	241925.218653	37.222618
1712.619417	242363.770333	37.227636
1713.996815	242807.578709	37.232653
1715.497460	243253.526708	37.237671
1717.502323	243705.336377	37.242688
1719.189134	244152.931682	37.247706
1720.969131	244603.408211	37.252724
1722.771222	245045.295662	37.257741
1724.531222	245491.534589	37.262759
1726.305714	245936.349204	37.267776
1727.718296	246398.853787	37.272794
1729.762805	246847.765699	37.277812
1731.643403	247296.578252	37.282829
1733.146597	247749.314951	37.287847
1735.354091	248195.508906	37.292864
1736.856761	248642.124629	37.297882
1738.966727	249095.575551	37.302900
1740.495061	249537.844071	37.307917
1742.471885	249980.191364	37.312935
1744.425214	250425.540517	37.317952
1745.867164	250880.983365	37.322970
1747.919763	251317.857657	37.327988
1750.077120	251752.327089	37.333005
1751.681047	252204.518059	37.338023
1753.524321	252631.952505	37.343040
1755.365747	253065.154053	37.348058
1757.214438	253479.099012	37.353076
1758.933360	253882.751907	37.358093
1760.564618	254282.507371	37.363111
1762.501461	254684.346403	37.368128
1764.008410	255103.861062	37.373146
1765.736867	255512.263457	37.378164
1767.738620	255914.295420	37.383181
1769.216658	256333.053148	37.388199
1770.684042	256745.004650	37.393216
1772.303098	257172.884451	37.398234
1774.134831	257596.969498	37.403252
1775.977940	258019.934967	37.408269
1777.528557	258449.401212	37.413287
1779.294222	258887.570682	37.418304
1780.880307	259320.536720	37.423322
1782.668449	259754.688710	37.428340
1784.538398	260195.076348	37.433357
1786.230670	260639.354557	37.438375
1788.108285	261074.736309	37.443392
1789.527284	261518.576777	37.448410
1791.474494	261969.087131	37.453428
1793.220747	262425.524067	37.458445
1795.059913	262889.007566	37.463463
1796.854426	263335.096999	37.468480
1798.461392	263798.618384	37.473498
1800.493665	264259.452722	37.478516
1802.620058	264713.488569	37.483533
1804.070220	265179.803916	37.488551
1806.124611	265637.178820	37.493568
1807.771048	266106.763440	37.498586
1809.547642	266569.543529	37.503604
1811.612081	267035.705076	37.508621
1813.562114	267504.196749	37.513639
1815.150595	267966.625528	37.518656
1816.676285	268441.257629	37.523674
1818.427339	268910.644358	37.528692
1820.564739	269390.458139	37.533709
1822.322114	269871.070761	37.538727
1824.148302	270351.010907	37.543744
1826.160103	270834.958787	37.548762
1828.024390	271309.582098	37.553780
1829.836123	271783.984764	37.558797
1831.510539	272278.782368	37.563815
1833.588608	272750.497657	37.568832
1835.128301	273237.517274	37.573850
1837.191741	273729.606268	37.578868
1838.998039	274212.693528	37.583885
1840.943136	274695.502948	37.588903
1842.749880	275179.985459	37.593920
1844.850056	275674.909748	37.598938
1846.718833	276161.513858	37.603956
1848.612462	276642.575147	37.608973
1850.037473	277130.571412	37.613991
1852.009854	277618.679416	37.619008
1853.719506	278110.640019	37.624026
1855.613089	278607.776514	37.629044
1857.762155	279083.887553	37.634061
1859.444627	279584.180954	37.639079
1861.359003	280071.149592	37.644096
1863.183452	280570.807338	37.649114
1865.212997	281051.251557	37.654132
1867.497341	281545.318528	37.659149
1869.112182	282040.155137	37.664167
1871.186263	282520.588037	37.669184
1873.014418	283011.246185	37.674202
1874.786755	283492.056377	37.679220
1876.837907	283980.642717	37.684237
1878.774056	284456.291941	37.689255
1880.738943	284921.647521	37.694272
1882.540230	285388.730596	37.699290
1884.379067	285851.005251	37.704308
1886.711346	286290.209159	37.709325
1887.957848	286766.473093	37.714343
1889.841806	287210.930044	37.719360
1891.995308	287691.079855	37.724378
1893.090852	288148.948615	37.729396
1895.278437	288629.445172	37.734413
1897.047176	289103.455895	37.739431
1899.167005	289567.526234	37.744448
1900.791974	290070.335814	37.749466
1902.249900	290536.518642	37.754484
1904.357091	291019.940779	37.759501
1906.149961	291509.000956	37.764519
1908.175732	291999.189138	37.769536
1909.969195	292489.845513	37.774554
1911.707025	292997.679229	37.779572
1913.600264	293493.547335	37.784589
1915.419095	294009.364166	37.789607
1917.759181	294502.639634	37.794624
1919.494959	295019.380007	37.799642
1921.072712	295520.828458	37.804660
1923.321186	296029.986754	37.809677
1925.131262	296562.454999	37.814695
1927.210292	297067.470993	37.819712
1929.121690	297593.237511	37.824730
1930.934648	298111.017134	37.829748
1932.780175	298617.181749	37.834765
1934.503941	299157.905510	37.839783
1936.387787	299686.027894	37.844800
1938.188979	300222.796416	37.849818
1939.833785	300768.045287	37.854836
1942.094591	301309.100349	37.859853
1944.174730	301855.083899	37.864871
1946.152939	302400.496985	37.869888
1948.211733	302938.477592	37.874906
1950.039129	303488.683849	37.879924
1951.990447	304036.631390	37.884941
1954.180093	304599.367927	37.889959
1956.375653	305137.795403	37.894976
1957.914605	305678.994621	37.899994
1960.014308	306243.767178	37.905012
1962.174678	306793.643890	37.910029
1963.905605	307352.654288	37.915047
1966.174992	307907.483328	37.920064
1967.949272	308447.178451	37.925082
1969.922116	309009.159798	37.930100
1972.071937	309567.476506	37.935117
1973.993609	310128.493475	37.940135
1976.169233	310682.734898	37.945152
1978.295518	311242.668961	37.950170
1980.320531	311800.279409	37.955188
1982.174019	312351.794095	37.960205
1984.080865	312912.996528	37.965223
1986.170236	313468.882691	37.970240
1988.181951	314025.209218	37.975258
1990.243642	314593.128150	37.980276
1992.181166	315151.337501	37.985293
1993.779356	315710.792046	37.990311
1995.927795	316272.792226	37.995328
1998.099532	316834.911060	38.000346
2000.134354	317404.614976	38.005364
2002.330681	317964.384533	38.010381
2004.203101	318529.509973	38.015399
2006.239341	319080.790464	38.020416
2008.295733	319651.919452	38.025434
2010.240611	320208.461859	38.030452
2012.355317	320742.957295	38.035469
2014.064756	321280.968484	38.040487
2016.275831	321820.390465	38.045504
2018.372310	322351.828797	38.050522
2019.894046	322894.148560	38.055540
2021.993936	323429.741377	38.060557
2023.870096	323973.973796	38.065575
2025.763840	324512.739760	38.070592
2028.028974	325056.543021	38.075610
2030.317264	325604.323771	38.080628
2032.150000	326156.237068	38.085645
2034.021726	326714.181440	38.090663
2036.035594	327263.820448	38.095680
2038.034788	327833.158201	38.100698
2039.933224	328396.464709	38.105716
2041.811964	328956.697102	38.110733
2043.773944	329534.021629	38.115751
2045.705418	330103.754563	38.120768
2047.750809	330682.551603	38.125786
2049.683995	331268.418805	38.130804
2051.746954	331848.648023	38.135821
2053.649260	332441.210105	38.140839
2055.653723	333037.099929	38.145856
2057.526659	333633.944265	38.150874
2059.084635	334244.110677	38.155892
2061.927293	334846.442515	38.160909
2063.979400	335456.234339	38.165927
2065.960833	336061.436205	38.170944
2068.159100	336676.139834	38.175962
2070.397570	337289.941151	38.180980
2072.479183	337897.795915	38.185997
2074.659961	338506.236326	38.191015
2076.881175	339132.024881	38.196032
2079.254906	339739.834861	38.201050
2081.042207	340350.450238	38.206068
2083.599277	340957.961337	38.211085
2085.881113	341569.114653	38.216103
2087.437372	342180.075579	38.221120
2090.018145	342798.423332	38.226138
2092.115647	343409.304834	38.231156
2094.299371	344017.600898	38.236173
2096.555335	344626.181848	38.241191
2098.764590	345246.107540	38.246208
2100.787328	345839.965592	38.251226
2102.976517	346463.685447	38.256244
2105.526881	347065.029180	38.261261
2107.709535	347676.729497	38.266279
2109.478148	348285.343084	38.271296
2112.197207	348883.031361	38.276314
2113.847338	349501.342552	38.281332
2116.173015	350110.296371	38.286349
2118.282880	350723.413931	38.291367
2120.186441	351324.985338	38.296384
2122.458571	351930.801625	38.301402
2124.358487	352549.612645	38.306420
2126.507003	353161.116407	38.311437
2128.822308	353770.376321	38.316455
2130.867556	354395.810505	38.321472
2133.464336	354989.857805	38.326490
2135.447008	355610.108031	38.331508
2137.787794	356208.925350	38.336525
2140.186242	356819.573895	38.341543
2142.116929	357420.166869	38.346560
2144.450652	358015.407067	38.351578
2146.350350	358627.202196	38.356596
2148.583118	359223.811553	38.361613
2150.836306	359833.297439	38.366631
2152.678161	360424.118157	38.371648
2155.117630	361002.323748	38.376666
2157.158950	361570.540010	38.381684
2159.490365	362146.818610	38.386701
2161.064204	362713.953925	38.391719
2163.745825	363282.293459	38.396736
2165.450971	363857.990636	38.401754
2167.505530	364442.399059	38.406772
2169.928870	365025.494694	38.411789
2171.806314	365606.160155	38.416807
2173.783145	366198.748351	38.421824
2176.079849	366788.078237	38.426842
2178.125389	367380.585803	38.431860
2179.968340	367971.214975	38.436877
2182.235907	368581.270902	38.441895
2184.435848	369184.910527	38.446912
2186.722655	369786.116255	38.451930
2188.360926	370411.185635	38.456948
2190.630559	371019.780297	38.461965
2192.968714	371648.010179	38.466983
2194.907532	372265.642511	38.472000
2197.277232	372890.446793	38.477018
2199.544954	373516.296800	38.482036
2201.745479	374146.052554	38.487053
2203.900441	374777.782754	38.492071
2206.239452	375423.318211	38.497088
2208.342039	376045.752057	38.502106
2210.417391	376705.382233	38.507124
2212.862380	377340.264038	38.512141
2214.924218	377981.384914	38.517159
2216.941839	378644.562913	38.522176
2219.930535	379294.406856	38.527194
2221.788961	379947.214160	38.532212
2224.110379	380579.976369	38.537229
2226.280644	381242.139733	38.542247
2228.485202	381900.785091	38.547264
2230.922344	382544.900918	38.552282
2233.048427	383215.450004	38.557300
2235.711339	383871.191112	38.562317
2238.111704	384527.038374	38.567335
2240.089770	385198.585099	38.572352
2242.080720	385851.303799	38.577370
2244.644788	386511.824522	38.582388
2247.180461	387175.048859	38.587405
2249.253831	387833.442785	38.592423
2251.591738	388498.573290	38.597440
2254.413956	389150.528985	38.602458
2256.682859	389822.183052	38.607476
2259.111675	390469.663741	38.612493
2261.482637	391122.134067	38.617511
2263.617011	391780.383587	38.622528
2265.977733	392428.290440	38.627546
2268.194068	393091.339480	38.632564
2270.853326	393744.441093	38.637581
2273.167967	394387.700492	38.642599
2275.250632	395046.850559	38.647616
2277.896079	395679.230406	38.652634
2280.541788	396331.973519	38.657652
2282.534003	396975.382187	38.662669
2284.855810	397618.671674	38.667687
2287.017086	398262.911175	38.672704
2289.561703	398892.121335	38.677722
2291.954733	399541.540009	38.682740
2294.278782	400179.577367	38.687757
2296.800226	400820.583460	38.692775
2298.641245	401469.112023	38.697792
2301.079979	402105.288311	38.702810
2303.084708	402736.428863	38.707828
2305.399306	403368.872395	38.712845
2307.770308	403981.377078	38.717863
2309.860764	404596.169621	38.722880
2312.267652	405212.365863	38.727898
2314.441104	405818.300572	38.732916
2316.464586	406437.902436	38.737933
2318.821365	407049.454883	38.742951
2321.122469	407683.271545	38.747968
2323.309477	408293.937430	38.752986
2325.421262	408923.095048	38.758004
2327.260617	409551.725659	38.763021
2329.925787	410189.679369	38.768039
2331.885968	410839.107918	38.773056
2334.288051	411481.279178	38.778074
2336.771214	412125.549236	38.783092
2339.056283	412792.126066	38.788109
2341.310953	413437.972191	38.793127
2343.682174	414111.795963	38.798144
2345.615725	414761.385617	38.803162
2348.092124	415428.344895	38.808180
2350.275506	416104.908590	38.813197
2352.540133	416779.769631	38.818215
2354.713550	417477.445543	38.823232
2356.876384	418153.781307	38.828250
2359.198595	418854.585783	38.833268
2361.527936	419549.013696	38.838285
2364.027554	420248.661336	38.843303
2366.169039	420957.818707	38.848320
2368.455427	421671.996133	38.853338
2370.959472	422376.774132	38.858356
2373.160362	423095.786084	38.863373
2375.598612	423813.877071	38.868391
2377.709044	424541.267369	38.873408
2380.414579	425266.056760	38.878426
2382.946487	425996.068308	38.883444
2385.346443	426726.687189	38.888461
2387.893384	427451.690480	38.893479
2389.725178	428199.369738	38.898496
2392.242014	428932.838567	38.903514
2394.820348	429671.286442	38.908532
2396.876522	430428.882223	38.913549
2399.873053	431166.353784	38.918567
2402.398459	431914.054439	38.923584
2404.856928	432661.033572	38.928602
2407.262493	433408.098693	38.933620
2409.556515	434162.497252	38.938637
2412.440456	434897.996392	38.943655
2414.876047	435652.828881	38.948672
2417.240263	436397.880576	38.953690
2420.174527	437133.805607	38.958708
2422.280866	437885.480737	38.963725
2424.858373	438613.926765	38.968743
2427.477534	439368.301678	38.973760
2429.986751	440105.414271	38.978778
2432.683324	440846.013560	38.983796
2435.168672	441596.388409	38.988813
2437.879918	442333.596099	38.993831
2440.101863	443073.693146	38.998848
2442.568026	443797.130470	39.003866
2445.292169	444536.133943	39.008884
2447.485673	445272.923352	39.013901
2449.967988	446005.744802	39.018919
2452.545237	446742.825519	39.023936
2454.949807	447462.457880	39.028954
2457.655158	448208.066452	39.033972
2459.977826	448938.841352	39.038989
2462.599957	449665.242484	39.044007
2465.152363	450392.844042	39.049024
2467.386505	451113.139541	39.054042
2470.192976	451806.714029	39.059060
2472.458977	452502.327020	39.064077
2475.023687	453189.725653	39.069095
2477.477856	453883.036335	39.074112
2479.848150	454579.068258	39.079130
2482.396681	455255.427865	39.084148
2484.734268	455958.750531	39.089165
2487.120877	456651.776849	39.094183
2489.632795	457349.511622	39.099200
2491.947705	458058.580074	39.104218
2494.411636	458749.701997	39.109236
2496.670678	459469.751564	39.114253
2499.294019	460181.475063	39.119271
2501.737456	460899.319684	39.124288
2504.070189	461622.969964	39.129306
2506.640282	462345.189962	39.134324
2509.110171	463066.692530	39.139341
2512.026407	463790.420116	39.144359
2514.448110	464529.567495	39.149376
2516.605092	465257.813983	39.154394
2519.248825	465994.898304	39.159412
2521.493979	466747.636229	39.164429
2524.196852	467495.771845	39.169447
2526.642885	468240.636248	39.174464
2528.990439	468988.620968	39.179482
2531.646012	469761.385737	39.184500
2533.860381	470534.545727	39.189517
2536.541090	471276.171168	39.194535
2539.289008	472065.449707	39.199552
2541.535786	472824.667850	39.204570
2544.385163	473592.950285	39.209588
2546.894453	474381.261765	39.214605
2549.827509	475148.708797	39.219623
2552.343128	475923.214226	39.224640
2554.327908	476706.917181	39.229658
2556.997788	477476.735781	39.234676
2559.632814	478272.891861	39.239693
2562.379350	479050.409748	39.244711
2564.997301	479845.237697	39.249728
2567.506378	480640.452910	39.254746
2570.513091	481432.319378	39.259764
2572.863909	482223.653430	39.264781
2575.406698	483011.083629	39.269799
2577.960388	483809.433841	39.274816
2580.324562	484610.203093	39.279834
2583.112955	485407.029468	39.284852
2585.490364	486208.936208	39.289869
2588.242411	487008.372182	39.294887
2590.747750	487831.133750	39.299904
2593.579007	488635.076284	39.304922
2595.859008	489442.202207	39.309940
2598.546104	490256.491525	39.314957
2601.340391	491068.605274	39.319975
2603.834763	491887.795760	39.324992
2606.157311	492693.400722	39.330010
2609.017021	493511.242530	39.335028
2611.702011	494325.239153	39.340045
2614.400698	495133.139799	39.345063
2616.968315	495950.559653	39.350080
2619.331125	496775.844437	39.355098
2622.463269	497591.073757	39.360116
2625.174143	498408.855432	39.365133
2627.417303	499228.591276	39.370151
2630.033591	500048.124454	39.375168
2632.694601	500872.048628	39.380186
2635.353711	501683.221904	39.385204
2637.774123	502509.525283	39.390221
2640.760438	503316.025137	39.395239
2643.535499	504111.627288	39.400256
2645.764831	504898.859332	39.405274
2648.149507	505683.708178	39.410292
2650.663374	506472.279526	39.415309
2653.608235	507258.270782	39.420327
2656.253514	508055.718061	39.425344
2658.372781	508861.178224	39.430362
2661.429678	509651.974767	39.435380
2663.574929	510455.938858	39.440397
2666.189603	511262.960643	39.445415
2668.632261	512074.405449	39.450432
2670.854027	512901.621116	39.455450
2673.704963	513727.228021	39.460468
2676.128102	514565.058275	39.465485
2678.584199	515409.238401	39.470503
2681.549539	516253.742411	39.475520
2684.006561	517095.865754	39.480538
2686.682606	517955.844775	39.485556
2689.121942	518814.706550	39.490573
2692.015764	519679.944572	39.495591
2694.777529	520546.717309	39.500608
2697.144370	521434.310912	39.505626
2699.866743	522308.596732	39.510644
2702.365101	523201.556100	39.515661
2705.408488	524085.458096	39.520679
2708.105480	524979.337322	39.525696
2710.628037	525885.782183	39.530714
2713.587722	526781.575470	39.535732
2716.312911	527683.547212	39.540749
2719.034802	528593.520949	39.545767
2721.958572	529497.665867	39.550784
2724.331555	530415.288325	39.555802
2727.114605	531321.660453	39.560820
2729.696092	532240.997138	39.565837
2732.537867	533170.551793	39.570855
2735.614537	534088.532669	39.575872
2737.874453	535030.697700	39.580890
2741.140529	535952.001935	39.585908
2743.977314	536878.149015	39.590925
2746.519745	537815.355113	39.595943
2749.474596	538743.676874	39.600960
2752.155607	539695.730849	39.605978
2754.994189	540629.080701	39.610996
2757.990598	541566.367469	39.616013
2761.065176	542504.132417	39.621031
2763.923852	543438.450104	39.626048
2766.280883	544379.326687	39.631066
2769.009633	545323.448174	39.636084
2772.062040	546267.150509	39.641101
2775.017339	547202.306409	39.646119
2778.040067	548140.605977	39.651136
2780.524118	549089.639828	39.656154
2783.204105	550027.364416	39.661172
2786.108222	550977.706516	39.666189
2788.896401	551927.096682	39.671207
2792.138939	552859.356131	39.676224
2794.761592	553807.787493	39.681242
2797.613466	554750.284534	39.686260
2800.716955	555688.603467	39.691277
2803.544376	556633.485101	39.696295
2806.313810	557563.034383	39.701312
2809.068874	558508.448386	39.706330
2811.947915	559446.087908	39.711348
2814.591317	560387.367116	39.716365
2817.531319	561328.982336	39.721383
2820.361528	562267.434007	39.726400
2823.148343	563214.163080	39.731418
2826.099117	564124.988188	39.736436
2828.758498	565039.413369	39.741453
2831.620870	565937.772263	39.746471
2834.693642	566830.259748	39.751488
2837.415712	567730.726405	39.756506
2839.733481	568627.431341	39.761524
2842.475073	569526.212520	39.766541
2845.185632	570436.581439	39.771559
2848.306403	571341.798274	39.776576
2851.080892	572258.149955	39.781594
2853.598490	573167.752678	39.786612
2856.471599	574090.228652	39.791629
2858.763219	575021.564470	39.796647
2862.156313	575935.389109	39.801664
2864.503208	576880.125061	39.806682
2867.490043	577816.857695	39.811700
2870.389384	578764.118825	39.816717
2873.379461	579717.713110	39.821735
2876.212688	580671.259643	39.826752
2878.661354	581647.765633	39.831770
2881.499092	582602.114561	39.836788
2884.543559	583574.908491	39.841805
2886.818567	584549.707205	39.846823
2890.043239	585528.031419	39.851840
2892.910270	586528.895249	39.856858
2895.666273	587512.650843	39.861876
2899.111081	588521.976324	39.866893
2901.656978	589516.830367	39.871911
2904.989121	590506.460462	39.876928
2907.484368	591511.230040	39.881946
2910.206434	592508.260984	39.886964
2913.128898	593544.255419	39.891981
2916.082654	594558.411011	39.896999
2919.373371	595573.225190	39.902016
2922.030402	596607.841654	39.907034
2925.144560	597628.016854	39.912052
2927.978368	598666.278400	39.917069
2930.861080	599702.586297	39.922087
2934.062125	600730.336872	39.927104
2936.342193	601776.572744	39.932122
2939.486304	602814.360704	39.937140
2942.977983	603863.761236	39.942157
2945.450124	604908.578547	39.947175
2948.780907	605955.811133	39.952192
2951.659954	607014.932314	39.957210
2954.473125	608074.315587	39.962228
2957.720673	609127.423507	39.967245
2960.463011	610185.269064	39.972263
2963.801698	611247.719004	39.977280
2966.501324	612303.770626	39.982298
2969.494515	613368.276586	39.987316
2972.690734	614432.847093	39.992333
2975.566435	615496.067905	39.997351
2978.434787	616566.137768	40.002368
2981.430370	617635.232617	40.007386
2984.473020	618703.565573	40.012404
2987.774287	619773.800945	40.017421
2990.339448	620847.201441	40.022439
2993.298433	621924.279186	40.027456
2996.440572	623003.168499	40.032474
2999.506212	624073.568036	40.037492
3002.559226	625150.058484	40.042509
3005.494088	626233.104677	40.047527
3008.587638	627302.128226	40.052544
3011.362105	628384.882590	40.057562
3014.351587	629466.492298	40.062580
3017.696461	630551.029023	40.067597
3020.400957	631643.499060	40.072615
3023.836205	632705.479570	40.077632
3026.769491	633752.358919	40.082650
3029.507315	634775.954333	40.087668
3032.558822	635813.422826	40.092685
3035.222224	636858.387719	40.097703
3038.409064	637892.032830	40.102720
3041.142057	638945.408557	40.107738
3043.832439	639997.835457	40.112756
3047.129938	641051.850363	40.117773
3049.963835	642113.714491	40.122791
3052.713317	643172.040645	40.127808
3055.703891	644249.068298	40.132826
3058.356364	645321.399883	40.137844
3061.414025	646407.412232	40.142861
3064.455892	647506.422127	40.147879
3067.148506	648601.531087	40.152896
3069.898470	649716.049842	40.157914
3073.031989	650835.016064	40.162932
3076.246871	651958.477651	40.167949
3079.212408	653089.377159	40.172967
3082.460791	654217.211235	40.177984
3085.454645	655360.650332	40.183002
3088.336087	656498.446197	40.188020
3092.039497	657639.709882	40.193037
3094.682052	658805.715125	40.198055
3098.205059	659946.390272	40.203072
3101.475440	661109.675721	40.208090
3104.469183	662266.793859	40.213108
3107.592050	663423.801819	40.218125
3110.588687	664606.969179	40.223143
3113.533958	665771.089490	40.228160
3116.658675	666950.164388	40.233178
3119.901356	668133.551513	40.238196
3123.283271	669314.380631	40.243213
3126.275777	670507.461639	40.248231
3129.640202	671690.185454	40.253248
3132.818941	672877.365968	40.258266
3135.986292	674073.148635	40.263284
3138.832548	675264.705260	40.268301
3142.328129	676459.134063	40.273319
3145.664242	677654.678143	40.278336
3148.864205	678864.252904	40.283354
3151.668499	680051.425258	40.288372
3155.534928	681255.011661	40.293389
3158.376948	682458.211693	40.298407
3161.846599	683652.259664	40.303424
3165.171000	684864.202010	40.308442
3168.402636	686064.230147	40.313460
3171.880508	687252.888175	40.318477
3175.232208	688466.925969	40.323495
3178.255075	689657.476716	40.328512
3181.440058	690848.239933	40.333530
3184.550155	692049.872951	40.338548
3188.325040	693240.021807	40.343565
3191.591186	694447.805196	40.348583
3194.869310	695637.565890	40.353600
3197.931708	696821.101998	40.358618
3200.946348	698012.421111	40.363636
3204.398184	699207.869816	40.368653
3207.685101	700403.331347	40.373671
3210.727671	701584.542938	40.378688
3214.102170	702776.294275	40.383706
3217.411917	703969.726232	40.388724
3220.468826	705158.823898	40.393741
3223.568033	706353.200214	40.398759
3226.901639	707540.437534	40.403776
3230.051184	708742.993116	40.408794
3233.187000	709928.099735	40.413812
3236.345473	711101.105493	40.418829
3239.824240	712258.797468	40.423847
3242.809387	713404.285518	40.428864
3246.256637	714541.376027	40.433882
3249.321014	715700.694336	40.438900
3252.467363	716836.732725	40.443917
3255.496469	717989.556004	40.448935
3258.706029	719137.689286	40.453952
3261.761172	720290.635782	40.458970
3264.446907	721454.115389	40.463988
3268.216209	722621.208734	40.469005
3270.869564	723796.231248	40.474023
3274.231854	724981.201574	40.479040
3277.719709	726156.886519	40.484058
3280.869870	727360.724514	40.489076
3284.114975	728561.009772	40.494093
3287.095273	729752.813056	40.499111
3290.309524	730958.776738	40.504128
3293.723810	732175.343689	40.509146
3296.744456	733383.447224	40.514164
3299.982369	734613.452408	40.519181
3302.748456	735857.465183	40.524199
3306.099683	737103.063866	40.529216
3309.592299	738346.668392	40.534234
3312.752603	739611.152699	40.539252
3316.409830	740857.741762	40.544269
3319.742604	742125.003228	40.549287
3322.789768	743397.977008	40.554304
3326.017024	744667.904513	40.559322
3329.531283	745946.551959	40.564340
3332.539320	747224.186481	40.569357
3335.880718	748522.946443	40.574375
3339.472840	749814.500059	40.579392
3342.927682	751115.074260	40.584410
3345.899710	752421.075504	40.589428
3349.625528	753710.921257	40.594445
3352.864802	755032.983552	40.599463
3356.248247	756344.011350	40.604480
3359.841623	757662.507937	40.609498
3363.266299	758979.032023	40.614516
3366.633423	760285.593668	40.619533
3370.351670	761602.449961	40.624551
3373.564076	762930.227904	40.629568
3376.890880	764243.292538	40.634586
3380.006452	765590.141816	40.639604
3383.528505	766900.544347	40.644621
3387.119668	768232.334264	40.649639
3390.688916	769576.323561	40.654656
3394.167308	770895.710660	40.659674
3397.242315	772229.815088	40.664692
3400.710556	773566.805855	40.669709
3404.242227	774901.578069	40.674727
3407.948443	776242.854345	40.679744
3411.478586	777582.194671	40.684762
3414.488361	778913.569432	40.689780
3418.063339	780242.545388	40.694797
3421.461164	781581.610451	40.699815
3425.189438	782924.395093	40.704832
3428.315920	784270.216183	40.709850
3431.524019	785618.811528	40.714868
3435.025408	786959.406095	40.719885
3438.319548	788314.636020	40.724903
3441.791507	789657.128872	40.729920
3445.634051	791001.854232	40.734938
3448.884796	792349.017559	40.739956
3452.058465	793698.482898	40.744973
3456.026307	795053.092009	40.749991
3459.458409	796409.485680	40.755008
3462.783872	797741.964459	40.760013
3465.920376	799025.928740	40.765018
3469.532983	800257.569955	40.770023
3472.511296	801433.124853	40.775028
3475.903954	802547.102644	40.780032
3479.079278	803574.234245	40.785037
3481.746044	804546.330471	40.790042
3484.695885	805443.526411	40.795047
3487.709175	806283.534762	40.800052
3489.893935	807040.643577	40.805056
3492.676203	807757.087920	40.810061
3494.667839	808393.562171	40.815066
3496.820973	808955.174960	40.820071
3499.305637	809486.994372	40.825076
3500.940600	809950.565923	40.830080
3503.133464	810343.712042	40.835085
3504.785869	810704.837010	40.840090
3506.568376	810988.376278	40.845095
3508.091338	811248.531860	40.850100
3509.564253	811443.146639	40.855104
3511.000315	811604.797142	40.860109
3512.035029	811726.051706	40.865114
3512.997843	811805.388816	40.870119
3514.575097	811858.958262	40.875124
3515.536435	811870.995932	40.880128
3516.297102	811842.903041	40.885133
3516.909441	811795.291282	40.890138
3518.095908	811715.404105	40.895143
3518.721249	811622.628290	40.900148
3519.539985	811492.200736	40.905152
3520.378836	811334.238495	40.910157
3520.581781	811161.730818	40.915162
3521.535606	810971.949782	40.920167
3522.112534	810757.584602	40.925172
3522.634167	810532.297065	40.930176
3522.851867	810278.980055	40.935181
3523.103492	810023.247310	40.940186
3523.420462	809733.491413	40.945191
3523.472254	809446.461692	40.950196
3523.813384	809151.777218	40.955200
3524.139383	808841.156863	40.960205
3524.039380	808536.914025	40.965210
3524.374175	808210.680101	40.970215
3524.821671	807888.724735	40.975220
3524.855082	807548.884311	40.980224
3525.261793	807203.818994	40.985229
3525.140660	806849.951261	40.990234
3525.064722	806490.959774	40.995239
3525.198275	806123.483215	41.000244
3525.639272	805760.103282	41.005248
3525.823198	805385.862485	41.010253
3525.350362	805006.463292	41.015258
3525.611985	804621.283364	41.020263
3525.754336	804237.866707	41.025268
3525.696147	803859.169280	41.030272
3525.952654	803455.290425	41.035277
3525.576467	803079.348669	41.040282
3525.300721	802677.277361	41.045287
3525.464582	802280.211217	41.050292
3525.419351	801895.272404	41.055296
3525.295573	801493.499380	41.060301
3525.038522	801105.559077	41.065306
3525.373023	800704.008006	41.070311
3525.342613	800302.493744	41.075316
3524.850539	799907.852389	41.080320
3524.666102	799513.088781	41.085325
3524.928846	799116.413368	41.090330
3525.017849	798723.375390	41.095335
3524.844551	798316.960384	41.100340
3524.679676	797927.501825	41.105344
3524.649410	797516.304792	41.110349
3524.246657	797134.596095	41.115354
3524.150308	796736.666024	41.120359
3524.344368	796338.910851	41.125364
3523.685789	795949.373958	41.130368
3524.029500	795557.048080	41.135373
3523.844693	795163.510698	41.140378
3523.616736	794771.676858	41.145383
3523.394583	794391.948979	41.150388
3523.227400	794010.570930	41.155392
3522.971197	793625.945558	41.160397
3522.714698	793252.545945	41.165402
3522.703229	792873.290523	41.170407
3522.774842	792495.179790	41.175412
3522.526820	792123.634433	41.180416
3522.672470	791743.064217	41.185421
3522.299386	791377.493140	41.190426
3522.344536	791007.805696	41.195431
3522.319105	790635.015290	41.200436
3522.175917	790272.149561	41.205440
3521.966578	789891.636329	41.210445
3521.676015	789537.208572	41.215450
3521.546058	789159.198100	41.220455
3521.344332	788800.787592	41.225460
3521.095298	788446.789914	41.230464
3521.173887	788090.115740	41.235469
3520.711947	787732.824618	41.240474
3520.618600	787383.270194	41.245479
3520.723988	787033.665860	41.250484
3520.237994	786688.664361	41.255488
3520.471404	786341.659528	41.260493
3520.139977	786007.365744	41.265498
3520.001057	785667.763918	41.270503
3520.049298	785318.871621	41.275508
3519.354402	784988.031756	41.280512
3519.463284	784651.094325	41.285517
3518.886066	784334.612285	41.290522
3518.954418	784014.026597	41.295527
3519.019758	783694.410652	41.300532
3518.356010	783371.900572	41.305536
3518.808135	783053.667802	41.310541
3518.725199	782737.328966	41.315546
3518.626303	782417.093040	41.320551
3518.744947	782105.857908	41.325556
3518.298440	781786.930158	41.330560
3518.364626	781462.443288	41.335565
3517.869004	781160.467808	41.340570
3517.926134	780840.234502	41.345575
3518.117377	780544.712648	41.350580
3517.564223	780247.628492	41.355584
3517.788682	779938.348950	41.360589
3517.567824	779637.691485	41.365594
3517.478018	779336.015775	41.370599
3517.324118	779028.924914	41.375604
3517.478027	778746.868709	41.380608
3517.187354	778442.285385	41.385613
3516.646930	778151.068106	41.390618
3516.784493	777858.841508	41.395623
3516.595384	777573.104865	41.400628
3516.520380	777297.330318	41.405632
3516.293191	777005.621777	41.410637
3515.955079	776737.006870	41.415642
3515.780555	776455.949683	41.420647
3516.053680	776177.417086	41.425652
3515.454420	775915.608663	41.430656
3515.582489	775637.768624	41.435661
3515.311501	775379.776343	41.440666
3515.450968	775112.746203	41.445671
3515.196239	774853.304799	41.450676
3514.979099	774588.825477	41.455680
3514.965032	774326.519045	41.460685
3514.732961	774076.500897	41.465690
3514.360253	773819.504515	41.470695
3514.362210	773571.449662	41.475700
3514.157566	773337.998157	41.480704
3514.473538	773079.434175	41.485709
3514.041905	772830.095965	41.490714
3513.966388	772595.269778	41.495719
3514.312877	772350.219936	41.500724
3513.897861	772102.479759	41.505728
3514.049079	771863.356752	41.510733
3513.841606	771627.339234	41.515738
3513.338144	771375.500577	41.520743
3513.796801	771150.195668	41.525748
3513.711428	770915.613167	41.530752
3513.401736	770676.773978	41.535757
3513.122071	770454.476240	41.540762
3513.406458	770226.462136	41.545767
3513.249409	769993.389538	41.550772
3512.704493	769771.065694	41.555776
3512.982142	769536.281079	41.560781
3512.833999	769321.712974	41.565786
3512.585667	769102.227451	41.570791
3512.882051	768874.317587	41.575796
3512.391870	768665.059656	41.580800
3512.633120	768438.081806	41.585805
3512.260297	768225.687413	41.590810
3512.328076	768017.649942	41.595815
3512.350544	767797.292674	41.600820
3511.921266	767593.711681	41.605824
3512.199714	767376.651303	41.610829
3512.167153	767174.373553	41.615834
3511.643701	766977.987564	41.620839
3511.661409	766757.008797	41.625844
3511.422310	766563.374711	41.630848
3511.318714	766362.614749	41.635853
3510.841894	766176.551968	41.640858
3510.942568	765980.381940	41.645863
3511.174659	765795.030906	41.650868
3510.798080	765617.072007	41.655872
3511.080890	765418.540111	41.660877
3510.911892	765243.742720	41.665882
3510.723440	765043.898058	41.670887
3510.666962	764850.436003	41.675892
3510.219082	764676.361586	41.680896
3510.539873	764491.456715	41.685901
3510.410656	764310.911303	41.690906
3510.385280	764131.379944	41.695911
3510.412988	763970.672391	41.700916
3510.167360	763793.141672	41.705920
3510.062775	763615.435572	41.710925
3510.250790	763429.934664	41.715930
3509.924048	763261.034782	41.720935
3509.937040	763092.913509	41.725940
3509.934506	762925.136261	41.730944
3509.816073	762748.496939	41.735949
3509.705954	762580.483137	41.740954
3509.872810	762416.267006	41.745959
3509.681779	762249.393537	41.750964
3509.503857	762088.778285	41.755968
3509.458987	761917.236974	41.760973
3509.452574	761746.523959	41.765978
3509.036074	761588.255658	41.770983
3509.042350	761439.779909	41.775988
3508.950332	761280.909090	41.780992
3508.828492	761128.699351	41.785997
3508.448661	760979.192911	41.791002
3508.739168	760833.963571	41.796007
3508.910087	760685.791193	41.801012
3508.647801	760538.081962	41.806016
3508.758537	760389.025683	41.811021
3508.603151	760237.691551	41.816026
3508.722634	760087.789195	41.821031
3508.605063	759947.395717	41.826036
3508.362163	759803.615943	41.831040
3508.691890	759652.831586	41.836045
3508.233628	759516.384060	41.841050
3508.131345	759371.438090	41.846055
3508.248070	759221.469712	41.851060
3507.995668	759094.701064	41.856064
3508.165961	758957.597139	41.861069
3508.181648	758823.920999	41.866074
3508.069771	758677.186940	41.871079
3508.128667	758539.748408	41.876084
3507.867085	758421.013505	41.881088
3507.818339	758275.593664	41.886093
3507.406045	758138.719002	41.891098
3507.653510	758009.727865	41.896103
3507.697038	757882.840880	41.901108
3507.579031	757753.560166	41.906112
3507.297119	757623.514624	41.911117
3507.546041	757499.499202	41.916122
3507.563321	757371.571602	41.921127
3507.535466	757248.041881	41.926132
3507.105242	757128.870403	41.931136
3507.300660	756992.220477	41.936141
3507.257695	756880.483501	41.941146
3507.269224	756761.924499	41.946151
3507.126091	756639.045561	41.951156
3506.889255	756519.388460	41.956160
3506.671551	756392.618428	41.961165
3506.913792	756283.293736	41.966170
3506.709348	756176.262366	41.971175
3506.810722	756058.368700	41.976180
3506.426555	755951.363791	41.981184
3506.836552	755834.353721	41.986189
3506.719129	755723.451271	41.991194
3506.691646	755614.704475	41.996199
3506.807713	755502.624945	42.001204
3506.752724	755397.680793	42.006208
3506.637486	755275.960142	42.011213
3506.642843	755168.386417	42.016218
3506.280717	755059.983089	42.021223
3506.199188	754950.199006	42.026228
3505.988299	754852.283569	42.031232
3506.274559	754746.780564	42.036237
3506.321508	754641.809257	42.041242
3506.103767	754540.237452	42.046247
3506.341465	754435.182515	42.051252
3505.895716	754342.483436	42.056256
3505.944324	754240.221911	42.061261
3505.646483	754145.422355	42.066266
3505.919790	754043.219932	42.071271
3506.048325	753947.508291	42.076276
3505.685338	753849.555736	42.081280
3505.736850	753753.014957	42.086285
3505.552523	753658.931351	42.091290
3505.524255	753571.289481	42.096295
3505.727820	753483.015861	42.101300
3505.686637	753389.152262	42.106304
3505.605397	753294.602791	42.111309
3505.991538	753209.160009	42.116314
3505.634647	753113.073536	42.121319
3505.575136	753013.677636	42.126324
3505.422861	752933.061198	42.131328
3505.650512	752837.023108	42.136333
3505.756062	752745.448495	42.141338
3505.264855	752659.600957	42.146343
3505.677589	752566.837761	42.151348
3505.073602	752485.698448	42.156352
3505.347265	752393.400551	42.161357
3505.181875	752300.334319	42.166362
3505.567259	752222.239347	42.171367
3505.586619	752133.931231	42.176372
3504.919246	752051.217372	42.181376
3505.573864	751956.629001	42.186381
3505.299792	751884.911676	42.191386
3505.122173	751794.705944	42.196391
3505.254977	751705.583991	42.201396
3505.151707	751632.008719	42.206400
3505.221814	751533.412020	42.211405
3504.840662	751464.622541	42.216410
3505.021141	751372.475968	42.221415
3505.130393	751295.207406	42.226420
3505.166987	751214.739452	42.231424
3504.961766	751140.237813	42.236429
3504.695002	751061.695231	42.241434
3504.910158	750982.627885	42.246439
3504.927079	750900.628651	42.251444
3504.986163	750823.956395	42.256448
3504.928360	750748.092987	42.261453
3505.020159	750669.190955	42.266458
3505.036419	750584.274042	42.271463
3505.138557	750506.356601	42.276468
3504.858001	750428.797828	42.281472
3505.331399	750349.236873	42.286477
3504.852246	750266.028276	42.291482
3504.689673	750190.571865	42.296487
3505.065351	750104.651864	42.301492
3504.678860	750042.322111	42.306496
3504.715703	749959.519208	42.311501
3504.740495	749887.141278	42.316506
3504.588588	749812.173447	42.321511
3504.602461	749738.709071	42.326516
3504.386271	749668.097915	42.331520
3504.387339	749593.794415	42.336525
3504.445209	749531.041500	42.341530
3504.390970	749458.919619	42.346535
3504.703671	749399.532590	42.351540
3504.590485	749325.640592	42.356544
3504.168298	749242.312800	42.361549
3504.322734	749177.219016	42.366554
3504.128258	749112.231586	42.371559
3504.510006	749041.269163	42.376564
3504.092604	748978.441872	42.381568
3504.266604	748912.107444	42.386573
3504.221955	748847.982466	42.391578
3503.896673	748774.861306	42.396583
3504.120108	748711.975674	42.401588
3504.091119	748665.584667	42.406592
3504.129497	748596.453523	42.411597
3504.108308	748544.773594	42.416602
3503.929644	748477.702998	42.421607
3504.352616	748412.509152	42.426612
3503.847728	748355.571214	42.431616
3504.083878	748281.908199	42.436621
3504.248449	748229.207316	42.441626
3503.935030	748156.720752	42.446631
3504.352999	748096.169924	42.451636
3503.887299	748039.272625	42.456640
3503.919774	747965.047205	42.461645
3504.302067	747910.232883	42.466650
3503.738317	747846.827579	42.471655
3504.203540	747790.417464	42.476660
3504.014863	747733.620529	42.481664
3503.918889	747669.889625	42.486669
3503.968015	747622.342954	42.491674
3503.895294	747556.680045	42.496679
3504.064592	747477.881074	42.501684
3503.496931	747431.176130	42.506688
3504.139819	747368.704716	42.511693
3504.121597	747311.876620	42.516698
3504.124410	747258.108617	42.521703
3504.194091	747182.683563	42.526708
3503.964626	747127.618611	42.531712
3504.087671	747065.032748	42.536717
3504.108283	747006.169800	42.541722
3504.039535	746939.710315	42.546727
3504.385798	746882.028295	42.551732
3504.001003	746821.056216	42.556736
3503.892392	746756.232652	42.561741
3503.946355	746698.745709	42.566746
3503.520885	746633.133152	42.571751
3503.659369	746581.759854	42.576756
3503.831074	746524.449921	42.581760
3503.836160	746464.300435	42.586765
3503.552221	746409.832481	42.591770
3503.490049	746362.790718	42.596775
3503.697504	746300.283670	42.601780
3503.414761	746244.331614	42.606784
3503.886959	746193.345605	42.611789
3503.707869	746145.530991	42.616794
3503.218981	746098.310820	42.621799
3503.632687	746039.968936	42.626804
3503.537606	745992.188967	42.631808
3503.913283	745936.620487	42.636813
3503.912104	745890.208387	42.641818
3503.231127	745831.402768	42.646823
3503.573295	745765.557579	42.651828
3503.376894	745726.343781	42.656832
3503.476044	745673.191569	42.661837
3503.437229	745614.921085	42.666842
3503.474209	745563.903836	42.671847
3503.675474	745509.794527	42.676852
3503.750452	745470.089859	42.681856
3503.552322	745402.155715	42.686861
3503.714666	745354.131711	42.691866
3503.598112	745308.526069	42.696871
3503.887422	745255.191395	42.701876
3503.782511	745194.555959	42.706880
3503.836949	745146.795626	42.711885
3503.579539	745084.454338	42.716890
3503.159616	745029.702582	42.721895
3503.345790	744984.094602	42.726900
3503.568421	744940.704860	42.731904
3503.639821	744883.893786	42.736909
3503.561965	744837.438649	42.741914
3503.669945	744777.110945	42.746919
3503.979070	744727.378143	42.751924
3503.454265	744670.268283	42.756928
3503.482360	744614.105049	42.761933
3503.515984	744568.173740	42.766938
3503.689836	744518.709086	42.771943
3503.707519	744468.528306	42.776948
3503.566645	744422.229405	42.781952
3503.568040	744364.733993	42.786957
3503.770521	744316.944216	42.791962
3503.423338	744260.691978	42.796967
3503.612620	744206.130716	42.801972
3503.337780	744159.753464	42.806977
3503.574149	744104.689354	42.811981
3503.284971	744042.493335	42.816986
3503.468541	743993.320409	42.821991
3503.784801	743947.141140	42.826996
3503.179256	743900.717971	42.832001
3503.545316	743847.311652	42.837005
3503.563866	743805.284161	42.842010
3503.138552	743754.133559	42.847015
3503.361714	743702.430799	42.852020
3503.254234	743667.888980	42.857025
3503.394967	743610.167322	42.862029
3503.421700	743565.862875	42.867034
3503.102661	743513.654910	42.872039
3503.426346	743468.954889	42.877044
3503.167623	743416.439682	42.882049
3503.244478	743363.769942	42.887053
3503.003357	743323.760405	42.892058
3503.464567	743275.377789	42.897063
3503.452102	743229.742920	42.902068
3503.086574	743185.945969	42.907073
3503.127131	743138.324049	42.912077
3503.322537	743088.846854	42.917082
3502.836562	743052.238555	42.922087
3503.036552	743003.650087	42.927092
3503.181108	742970.497604	42.932097
3503.378198	742918.793997	42.937101
3503.269075	742885.435725	42.942106
3502.782468	742845.216973	42.947111
3502.886620	742796.890256	42.952116
3502.971180	742762.906186	42.957121
3502.839969	742707.843431	42.962125
3503.090668	742673.831602	42.967130
3502.764566	742638.530125	42.972135
3502.922727	742589.006483	42.977140
3502.628701	742560.275995	42.982145
3502.796711	742517.376379	42.987149
3502.875635	742480.177848	42.992154
3502.753192	742442.517830	42.997159
3503.343775	742403.454455	43.002164
3502.926413	742368.661301	43.007169
3502.803309	742318.292211	43.012173
3502.787335	742272.751280	43.017178
3503.149459	742239.015920	43.022183
3503.082055	742190.763211	43.027188
3502.863196	742163.057356	43.032193
3503.026712	742105.419830	43.037197
3503.042860	742067.685734	43.042202
3502.964619	742029.324138	43.047207
3503.343584	741992.271677	43.052212
3502.871712	741951.600864	43.057217
3503.072110	741903.697891	43.062221
3503.196276	741870.099073	43.067226
3503.110871	741823.330669	43.072231
3503.071710	741771.460664	43.077236
3503.094735	741733.427119	43.082241
3503.007829	741685.669073	43.087245
3503.046258	741651.391097	43.092250
3503.162463	741610.918352	43.097255
3503.078809	741558.559736	43.102260
3502.916741	741522.830596	43.107265
3502.999507	741476.873166	43.112269
3502.895031	741435.496235	43.117274
3502.866040	741395.639780	43.122279
3502.993881	741345.371502	43.127284
3502.968366	741319.510160	43.132289
3502.921169	741266.105019	43.137293
3503.119984	741231.699883	43.142298
3502.892299	741198.106730	43.147303
3502.994924	741158.623050	43.152308
3502.821580	741122.349927	43.157313
3502.963129	741080.040362	43.162317
3503.015598	741035.915301	43.167322
3502.940130	741004.126191	43.172327
3503.196519	740958.879018	43.177332
3502.832388	740924.070721	43.182337
3502.784533	740869.377082	43.187341
3503.095916	740828.620881	43.192346
3502.857850	740794.434212	43.197351
3503.170624	740748.632493	43.202356
3502.977359	740712.509153	43.207361
3503.245992	740665.032582	43.212365
3502.887393	740624.781413	43.217370
3503.063029	740589.585939	43.222375
3502.935637	740553.549941	43.227380
3502.859883	740511.421530	43.232385
3502.791122	740465.878891	43.237389
3502.811983	740408.598744	43.242394
3502.666720	740388.541141	43.247399
3502.795238	740363.690001	43.252404
3503.152370	740322.824738	43.257409
3502.838475	740279.151531	43.262413
3503.242694	740244.312563	43.267418
3502.908564	740207.468186	43.272423
3502.987247	740158.882231	43.277428
3502.854848	740124.230084	43.282433
3502.859164	740079.612997	43.287437
3502.935059	740030.680468	43.292442
3502.726765	740009.494612	43.297447
3502.869127	739962.034641	43.302452
3502.717682	739923.922224	43.307457
3502.907973	739891.985931	43.312461
3503.150953	739843.222576	43.317466
3502.968472	739809.368755	43.322471
3503.136843	739762.002235	43.327476
3502.724409	739726.603038	43.332481
3503.113200	739680.535300	43.337485
3503.188940	739627.593525	43.342490
3502.986073	739605.366891	43.347495
3502.973048	739561.887491	43.352500
3502.727366	739524.876965	43.357505
3502.646974	739476.065706	43.362509
3502.919129	739445.449759	43.367514
3502.598859	739408.500449	43.372519
3502.692046	739371.235495	43.377524
3502.763157	739335.754877	43.382529
3502.412191	739302.223466	43.387533
3503.145400	739257.283778	43.392538
3502.916272	739227.837915	43.397543
3502.599118	739190.738670	43.402548
3502.654335	739155.507214	43.407553
3502.625287	739119.003267	43.412557
3502.771517	739081.678747	43.417562
3502.455152	739050.564612	43.422567
3502.859295	739008.002852	43.427572
3502.649007	738976.128886	43.432577
3502.860339	738933.202729	43.437581
3502.884234	738901.685647	43.442586
3502.584495	738870.518597	43.447591
3502.936329	738824.946712	43.452596
3502.690533	738784.519197	43.457601
3502.811715	738755.112803	43.462605
3502.732768	738716.191089	43.467610
3502.669823	738689.585253	43.472615
3502.831785	738644.093093	43.477620
3502.715459	738626.549389	43.482625
3502.549519	738573.838313	43.487629
3502.741686	738541.995239	43.492634
3502.408398	738515.631262	43.497639
3502.799711	738471.287694	43.502644
3502.547307	738446.097536	43.507649
3502.560099	738396.472708	43.512653
3502.485227	738360.517052	43.517658
3502.385645	738336.538233	43.522663
3502.732123	738302.343455	43.527668
3502.416587	738257.570945	43.532673
3502.332703	738232.006012	43.537677
3502.618194	738198.810351	43.542682
3502.643388	738176.096857	43.547687
3502.860875	738130.048379	43.552692
3502.594853	738090.560718	43.557697
3502.521933	738064.053388	43.562701
3502.519145	738024.324117	43.567706
3502.560796	737991.365679	43.572711
3502.889489	737958.656671	43.577716
3502.503666	737924.729374	43.582721
3502.464878	737890.249972	43.587725
3502.629601	737867.017830	43.592730
3502.567435	737843.476661	43.597735
3502.563569	737808.644807	43.602740
3502.461782	737781.151730	43.607745
3502.438754	737734.546861	43.612749
3502.682423	737697.793548	43.617754
3502.744871	737675.765194	43.622759
3502.720855	737636.532279	43.627764
3502.860037	737600.092609	43.632769
3502.547062	737564.172594	43.637773
3502.776654	737526.876537	43.642778
3502.568464	737505.535547	43.647783
3502.656978	737457.723162	43.652788
3502.375736	737429.219355	43.657793
3502.662423	737396.168602	43.662797
3502.721918	737357.068995	43.667802
3502.865863	737334.630424	43.672807
3502.843503	737286.686841	43.677812
3502.614315	737263.864222	43.682817
3502.695157	737216.249582	43.687821
3502.386532	737180.920905	43.692826
3502.414200	737144.992354	43.697831
3502.562264	737108.153118	43.702836
3502.693682	737099.472071	43.707841
3502.481514	737062.939397	43.712845
3502.574173	737025.168736	43.717850
3502.346422	737005.066705	43.722855
3502.423268	736960.568635	43.727860
3502.536895	736944.566805	43.732865
3502.219562	736903.498247	43.737869
3502.665520	736880.167413	43.742874
3502.190762	736843.231647	43.747879
3502.550035	736806.950031	43.752884
3502.481205	736781.427453	43.757889
3502.475355	736753.519152	43.762893
3502.576891	736709.807374	43.767898
3502.443335	736696.171570	43.772903
3502.637769	736655.017407	43.777908
3502.664693	736622.501115	43.782913
3502.443021	736583.394568	43.787917
3502.552123	736547.152997	43.792922
3502.518152	736531.817981	43.797927
3502.222776	736486.537345	43.802932
3502.331743	736463.557745	43.807937
3502.736190	736426.079285	43.812941
3502.925309	736402.442976	43.817946
3502.334339	736361.713642	43.822951
3502.791481	736322.741403	43.827956
3502.837259	736285.816261	43.832961
3502.444775	736256.435820	43.837965
3502.408764	736232.440203	43.842970
3502.437048	736199.822994	43.847975
3502.745462	736166.169726	43.852980
3502.468989	736143.500162	43.857985
3502.441517	736106.239842	43.862989
3502.392467	736064.132990	43.867994
3502.496898	736036.599929	43.872999
3502.589632	735999.368794	43.878004
3502.671309	735968.770910	43.883009
3502.711240	735940.703762	43.888013
3502.795135	735897.930764	43.893018
3502.728688	735863.249215	43.898023
3502.682638	735832.919309	43.903028
3502.507162	735805.431576	43.908033
3502.526894	735769.448666	43.913037
3502.848502	735728.862681	43.918042
3502.512057	735700.757729	43.923047
3502.386742	735656.681654	43.928052
3502.848321	735630.573093	43.933057
3502.641458	735586.658545	43.938061
3502.585732	735554.992901	43.943066
3502.377849	735530.578073	43.948071
3502.787668	735486.264407	43.953076
3502.369753	735457.875072	43.958081
3502.279539	735440.270568	43.963085
3502.508588	735402.816232	43.968090
3502.570225	735373.852649	43.973095
3502.785129	735340.854742	43.978100
3502.948610	735313.952885	43.983105
3502.484490	735274.285968	43.988109
3502.854160	735243.142923	43.993114
3502.498894	735208.951580	43.998119
3502.605728	735170.922370	44.003124
3502.850417	735132.622790	44.008129
3502.529973	735101.493922	44.013133
3502.746316	735049.340036	44.018138
3502.550207	735039.077388	44.023143
3502.887868	734995.713318	44.028148
3502.806463	734961.822263	44.033153
3502.569924	734920.433240	44.038157
3502.378928	734883.491160	44.043162
3502.342633	734858.947020	44.048167
3502.634270	734821.331171	44.053172
3502.279649	734796.938288	44.058177
3502.471561	734767.109606	44.063181
3502.450686	734736.177442	44.068186
3502.508420	734709.538472	44.073191
3502.646474	734670.561300	44.078196
3502.593427	734639.733061	44.083201
3502.388570	734615.958420	44.088205
3502.656582	734581.166720	44.093210
3502.545811	734554.555002	44.098215
3502.468353	734520.562439	44.103220
3502.504849	734486.600454	44.108225
3502.522259	734453.482951	44.113229
3502.347082	734423.911480	44.118234
3502.227547	734390.667787	44.123239
3502.120177	734367.717834	44.128244
3502.288456	734344.969894	44.133249
3502.190781	734313.207264	44.138253
3502.419691	734283.469692	44.143258
3502.170012	734266.235389	44.148263
3502.401166	734228.527736	44.153268
3502.419104	734198.527612	44.158273
3502.250932	734174.993123	44.163277
3502.861643	734133.806943	44.168282
3502.265741	734108.065699	44.173287
3502.562448	734066.683410	44.178292
3502.444569	734038.437614	44.183297
3502.422677	734008.393843	44.188301
3502.260777	733978.620539	44.193306
3502.263246	733949.859583	44.198311
3502.247504	733921.596546	44.203316
3501.947488	733894.122786	44.208321
3502.081251	733874.052328	44.213325
3502.310057	733833.373065	44.218330
3502.444981	733813.500275	44.223335
3502.222161	733782.993744	44.228340
3502.283474	733768.231780	44.233345
3502.293428	733736.944171	44.238349
3502.310781	733716.644987	44.243354
3502.320714	733688.327397	44.248359
3502.556229	733655.764716	44.253364
3502.126416	733630.390602	44.258369
3502.228405	733589.582493	44.263373
3502.309003	733570.411115	44.268378
3502.378594	733547.677186	44.273383
3502.284283	733518.980142	44.278388
3502.388407	733488.319611	44.283393
3502.117534	733461.087094	44.288397
3502.526972	733417.999732	44.293402
3502.030853	733402.338846	44.298407
3502.213109	733374.734339	44.303412
3502.630478	733346.397917	44.308417
3502.008475	733320.707954	44.313421
3502.122473	733289.450969	44.318426
3502.128565	733264.993995	44.323431
3501.981056	733249.324873	44.328436
3502.334845	733222.978746	44.333441
3502.246771	733192.992346	44.338445
3502.219363	733152.698414	44.343450
3502.130293	733139.890848	44.348455
3502.388385	733110.985762	44.353460
3502.568735	733084.964807	44.358465
3502.113708	733048.503370	44.363469
3502.498318	733019.527603	44.368474
3502.004147	733002.875462	44.373479
3502.371466	732964.842416	44.378484
3502.215742	732941.054727	44.383489
3502.084201	732932.858089	44.388493
3502.514769	732899.864153	44.393498
3502.314626	732872.865534	44.398503
3502.516911	732843.968690	44.403508
3502.467221	732810.013838	44.408513
3502.010457	732785.978243	44.413517
3502.297861	732757.710682	44.418522
3502.001903	732731.271979	44.423527
3502.661571	732696.209574	44.428532
3502.568578	732671.717619	44.433537
3502.509995	732638.506159	44.438541
3502.414971	732604.359873	44.443546
3502.174630	732590.932727	44.448551
3502.281311	732548.237187	44.453556
3502.397995	732527.275005	44.458561
3502.289192	732496.051662	44.463565
3502.340542	732472.228470	44.468570
3502.021284	732440.940570	44.473575
3502.144601	732420.373107	44.478580
3502.365139	732388.302898	44.483585
3502.287442	732359.896062	44.488589
3502.713178	732329.326671	44.493594
3502.157185	732295.354059	44.498599
3502.327776	732266.163298	44.503604
3502.480837	732234.153109	44.508609
3502.203924	732212.809355	44.513613
3502.454668	732170.880286	44.518618
3502.452685	732156.373370	44.523623
3502.364223	732116.529945	44.528628
3502.532031	732098.083400	44.533633
3502.387393	732079.044623	44.538637
3502.451189	732028.530275	44.543642
3502.197701	732012.826700	44.548647
3502.270704	731979.046194	44.553652
3502.364712	731956.204733	44.558657
3502.175024	731923.160478	44.563661
3502.544107	731904.977415	44.568666
3501.999960	731882.438958	44.573671
3502.173736	731837.648995	44.578676
3502.241401	731819.465892	44.583681
3502.059561	731796.075252	44.588685
3502.376719	731762.550703	44.593690
3502.076223	731750.171892	44.598695
3502.572323	731709.289344	44.603700
3502.662930	731686.051556	44.608705
3502.361460	731656.540257	44.613709
3502.414976	731619.641951	44.618714
3502.199187	731590.561938	44.623719
3502.302905	731551.377292	44.628724
3502.283286	731536.822654	44.633729
3502.134167	731495.847280	44.638733
3502.583837	731479.284046	44.643738
3502.470368	731457.416192	44.648743
3502.043406	731420.546634	44.653748
3502.107921	731389.835152	44.658753
3502.216343	731364.414728	44.663757
3502.275729	731336.575923	44.668762
3502.238174	731314.596138	44.673767
3502.723061	731293.966236	44.678772
3502.466199	731268.358110	44.683777
3502.375692	731241.732120	44.688781
3502.485302	731208.635629	44.693786
3502.284810	731184.453994	44.698791
3502.455392	731143.523195	44.703796
3502.341364	731111.404022	44.708801
3502.384330	731091.143541	44.713805
3502.515338	731057.943870	44.718810
3502.186540	731033.931486	44.723815
3502.445907	730999.175308	44.728820
3502.526829	730971.678342	44.733825
3502.610204	730946.013132	44.738829
3502.552328	730900.959042	44.743834
3502.766415	730880.620317	44.748839
3502.341660	730838.449016	44.753844
3502.270911	730813.551600	44.758849
3502.596274	730785.221384	44.763853
3502.804636	730748.095510	44.768858
3502.462631	730720.914991	44.773863
3502.488656	730689.761504	44.778868
3502.501710	730654.103519	44.783873
3502.268597	730638.542482	44.788877
3502.106793	730591.324816	44.793882
3502.219028	730574.815344	44.798887
3502.207576	730548.867368	44.803892
3502.170464	730520.992142	44.808897
3502.028923	730495.956846	44.813901
3502.374770	730467.275485	44.818906
3502.074601	730441.671881	44.823911
3502.230289	730419.063544	44.828916
3502.405938	730389.716624	44.833921
3502.128577	730371.339508	44.838925
3502.148398	730334.242810	44.843930
3501.765422	730315.932495	44.848935
3502.271287	730289.304157	44.853940
3502.098193	730266.700048	44.858945
3502.056125	730247.640061	44.863949
3502.611500	730210.305976	44.868954
3502.021867	730188.463633	44.873959
3501.855435	730165.560995	44.878964
3502.313027	730138.296290	44.883969
3501.892899	730111.968531	44.888973
3502.060516	730097.727136	44.893978
3502.045295	730067.370467	44.898983
3502.012777	730044.940679	44.903988
3502.278402	730016.370000	44.908993
3502.100134	729998.669075	44.913997
3502.357963	729955.142549	44.919002
3501.743355	729949.597856	44.924007
3501.594200	729934.467370	44.929012
3502.234718	729891.521291	44.934017
3501.849223	729880.292738	44.939021
3502.191367	729845.468459	44.944026
3502.037184	729838.609644	44.949031
3502.520399	729803.860997	44.954036
3502.044756	729793.092923	44.959041
3502.274970	729767.251212	44.964045
3502.485011	729730.516635	44.969050
3502.353671	729706.022028	44.974055
3502.178883	729666.725592	44.979060
3502.321631	729637.282323	44.984065
3502.054195	729627.371230	44.989069
3502.234275	729594.900421	44.994074
3502.215185	729583.462495	44.999079
3502.607493	729545.756005	45.004084
3501.950642	729530.114075	45.009089
3502.068355	729494.532814	45.014093
3502.323088	729474.629640	45.019098
3502.237927	729448.393120	45.024103
3502.215211	729424.820827	45.029108
3501.768219	729389.579806	45.034113
3502.048351	729377.547457	45.039117
3502.165048	729339.588248	45.044122
3502.299694	729330.254430	45.049127
3502.354609	729298.744140	45.054132
3502.260360	729271.914183	45.059137
3501.972812	729243.184289	45.064141
3502.353731	729221.427066	45.069146
3502.191675	729198.421918	45.074151
3501.992887	729166.110891	45.079156
3502.370070	729131.079662	45.084161
3502.170757	729115.559663	45.089165
3502.403647	729085.009850	45.094170
3502.101754	729064.305824	45.099175
3502.307320	729031.085591	45.104180
3502.056258	729011.710420	45.109185
3502.008198	728978.878491	45.114189
3502.171560	728950.519054	45.119194
3501.940980	728932.428166	45.124199
3501.755859	728906.503565	45.129204
3502.148967	728885.535964	45.134209
3501.938261	728856.593911	45.139213
3502.115430	728837.345895	45.144218
3502.295276	728818.939458	45.149223
3502.212057	728791.065899	45.154228
3502.268370	728767.231013	45.159233
3501.880848	728755.159161	45.164237
3502.080204	728722.533099	45.169242
3502.139918	728706.276162	45.174247
3502.200791	728673.573655	45.179252
3502.161027	728657.877891	45.184257
3501.786104	728629.655571	45.189261
3502.218602	728591.442703	45.194266
3501.836676	728585.908258	45.199271
3502.317619	728552.640700	45.204276
3501.881768	728531.858321	45.209281
3501.788216	728501.360113	45.214285
3501.973082	728484.487689	45.219290
3501.934930	728476.469289	45.224295
3501.757542	728444.052799	45.229300
3501.999926	728420.334846	45.234305
3501.630092	728403.008763	45.239309
3501.843315	728373.202563	45.244314
3502.135363	728375.433147	45.249319
3501.914035	728339.407349	45.254324
3502.518933	728326.923650	45.259329
3501.932094	728299.874441	45.264333
3502.387419	728269.185849	45.269338
3501.898989	728253.315553	45.274343
3502.019343	728223.524110	45.279348
3502.062843	728195.924857	45.284353
3501.863596	728169.207644	45.289357
3502.127138	728149.993312	45.294362
3501.902902	728136.655199	45.299367
3501.908140	728108.269354	45.304372
3502.188696	728091.677578	45.309377
3502.251697	728066.848789	45.314381
3502.268653	728034.745414	45.319386
3502.189813	728005.134613	45.324391
3501.891289	727980.959594	45.329396
3502.176774	727952.328875	45.334401
3502.084263	727945.061988	45.339405
3502.008334	727916.589775	45.344410
3502.060765	727910.388828	45.349415
3502.275344	727883.751108	45.354420
3502.542696	727849.624184	45.359425
3502.084911	727826.168498	45.364429
3502.218740	727792.608271	45.369434
3502.009933	727767.971981	45.374439
3501.933058	727744.849613	45.379444
3501.997915	727725.369784	45.384449
3501.788580	727699.247174	45.389453
3502.012767	727688.410523	45.394458
3501.833389	727657.378361	45.399463
3501.880460	727643.301169	45.404468
3502.043079	727609.537285	45.409473
3501.885031	727598.416714	45.414477
3502.040735	727582.637132	45.419482
3502.073392	727554.492549	45.424487
3502.374759	727524.321945	45.429492
3502.196181	727495.667013	45.434497
3501.933336	727483.374561	45.439501
3502.347775	727440.205145	45.444506
3501.971016	727434.025017	45.449511
3501.926174	727406.437654	45.454516
3502.312763	727377.391930	45.459521
3501.892177	727354.374634	45.464525
3502.333094	727328.540029	45.469530
3502.152516	727307.811546	45.474535
3501.843312	727284.478445	45.479540
3501.975666	727269.147990	45.484545
3501.919398	727229.820275	45.489549
3502.206770	727213.671485	45.494554
3502.320912	727194.925419	45.499559
3502.147724	727164.633513	45.504564
3502.619036	727132.897619	45.509569
3501.701752	727117.194857	45.514573
3502.303642	727089.351227	45.519578
3502.026659	727067.795775	45.524583
3501.627938	727042.990416	45.529588
3501.890166	727019.562398	45.534593
3502.042642	727018.794158	45.539597
3502.171230	726979.137512	45.544602
3502.282490	726962.472258	45.549607
3502.235582	726944.544869	45.554612
3502.135484	726915.478615	45.559617
3501.858270	726884.806454	45.564621
3502.147529	726857.310822	45.569626
3502.035094	726836.817643	45.574631
3501.921560	726812.113225	45.579636
3501.812912	726803.510253	45.584641
3501.837148	726775.067104	45.589645
3502.173805	726752.468337	45.594650
3502.380289	726732.219620	45.599655
3502.133193	726703.573203	45.604660
3501.955976	726669.266885	45.609665
3502.104750	726656.806269	45.614669
3502.378620	726634.019336	45.619674
3502.145194	726602.942531	45.624679
3502.278038	726582.953314	45.629684
3502.037934	726550.242361	45.634689
3501.901380	726534.954843	45.639693
3502.117970	726499.393791	45.644698
3502.157599	726479.617871	45.649703
3501.945536	726455.671826	45.654708
3502.016107	726431.778235	45.659713
3502.102061	726413.629601	45.664717
3502.228177	726384.573734	45.669722
3502.094181	726360.515451	45.674727
3502.218608	726340.873869	45.679732
3502.173742	726313.976505	45.684737
3501.910849	726294.249988	45.689741
3502.204161	726274.976808	45.694746
3502.177081	726259.323896	45.699751
3502.127745	726246.052970	45.704756
3501.900740	726202.635893	45.709761
3502.109964	726195.862772	45.714765
3502.185707	726155.318963	45.719770
3502.296744	726150.742160	45.724775
3501.931222	726108.932996	45.729780
3502.071975	726092.954812	45.734785
3501.960858	726069.486503	45.739789
3502.265470	726046.147824	45.744794
3502.383142	726014.218129	45.749799
3501.897179	725999.185387	45.754804
3502.206686	725967.124798	45.759809
3501.759135	725941.878187	45.764813
3502.006817	725896.746097	45.769818
3501.659005	725827.778562	45.774823
3501.927150	725681.457210	45.779828
3501.722970	725499.978663	45.784833
3501.537583	725246.935951	45.789837
3501.661547	724942.692018	45.794842
3501.044740	724592.518803	45.799847
3500.881940	724174.357008	45.804852
3500.657938	723698.441892	45.809857
3500.103609	723174.622191	45.814861
3499.868115	722595.346220	45.819866
3499.921848	721966.952832	45.824871
3499.687880	721266.223971	45.829876
3499.109018	720503.761672	45.834881
3498.364353	719684.379203	45.839885
3498.325643	718803.700818	45.844890
3497.537510	717877.521271	45.849895
3496.967259	716881.062247	45.854900
3496.409091	715824.850473	45.859905
3495.461738	714727.040340	45.864909
3494.969580	713552.888609	45.869914
3494.411204	712328.605827	45.874919
3493.483000	711030.145833	45.879924
3492.436573	709689.207989	45.884929
3491.212856	708287.906855	45.889933
3490.573307	706827.975331	45.894938
3489.432304	705315.772442	45.899943
3488.428598	703748.980438	45.904948
3487.379143	702117.066575	45.909953
3486.187635	700440.289052	45.914957
3484.741520	698700.547481	45.919962
3483.715326	696922.206835	45.924967
3482.709085	695074.180071	45.929972
3481.340062	693167.182823	45.934977
3479.822847	691226.616875	45.939981
3478.267741	689213.629098	45.944986
3476.851735	687185.434540	45.949991
3475.301877	685082.377255	45.954996
3473.953821	682935.028013	45.960001
3472.039593	680742.588463	45.965005
3470.629524	678489.607490	45.970010
3469.231864	676210.710064	45.975015
3467.424995	673868.565256	45.980020
3465.915231	671489.139022	45.985025
3463.818376	669056.593719	45.990029
3462.571305	666575.594319	45.995034
3460.310161	664057.042952	46.000039
3458.511619	661486.047170	46.005044
3456.378604	658875.382315	46.010049
3454.775171	656242.906869	46.015053
3452.648034	653547.521995	46.020058
3450.484051	650813.134959	46.025063
3448.591062	648041.517958	46.030068
3446.242103	645228.416610	46.035073
3443.918963	642388.725377	46.040077
3441.905948	639488.066979	46.045082
3439.856685	636574.588173	46.050087
3437.658949	633608.564138	46.055092
3435.352682	630622.792954	46.060097
3432.741660	627600.120820	46.065101
3430.301581	624522.812927	46.070106
3428.135243	621415.165591	46.075111
3425.387684	618282.765290	46.080116
3423.327032	615110.850813	46.085121
3420.378942	611911.742786	46.090125
3418.059622	608680.611874	46.095130
3415.074331	605425.380936	46.100135
3412.583714	602128.279612	46.105140
3410.076669	598803.072856	46.110145
3407.372561	595440.033187	46.115149
3404.781285	592055.916815	46.120154
3401.966445	588646.098401	46.125159
3399.106686	585209.632593	46.130164
3396.418873	581742.751314	46.135169
3393.429581	578256.733756	46.140173
3390.684018	574735.235785	46.145178
3387.477895	571196.320579	46.150183
3384.532583	567631.913450	46.155188
3381.690794	564039.010318	46.160193
3378.825227	560438.975529	46.165197
3375.910214	556804.515134	46.170202
3372.795897	553147.833332	46.175207
3369.799926	549472.804398	46.180212
3366.717311	545764.637448	46.185217
3362.969835	542049.185690	46.190221
3360.193295	538300.914066	46.195226
3356.813958	534540.354600	46.200231
3353.671174	530773.379541	46.205236
3350.793749	526977.830576	46.210241
3347.292931	523172.278379	46.215245
3343.901426	519328.171781	46.220250
3340.526349	515487.799620	46.225255
3337.263556	511632.061478	46.230260
3334.420136	507754.238237	46.235265
3330.563561	503874.030724	46.240269
3327.637861	499957.754756	46.245274
3323.782012	496037.271257	46.250279
3320.379777	492110.593946	46.255284
3316.923054	488160.510684	46.260289
3313.417584	484213.038095	46.265293
3310.438595	480237.671056	46.270298
3306.328583	476252.303315	46.275303
3302.698848	472262.301180	46.280308
3299.176544	468253.351711	46.285313
3295.383297	464256.735744	46.290317
3292.162876	460237.012757	46.295322
3288.428726	456211.244988	46.300327
3285.044770	452176.615821	46.305332
3281.000754	448139.287376	46.310337
3277.319954	444094.541195	46.315341
3273.836241	440033.590221	46.320346
3270.165650	435982.941211	46.325351
3266.235447	431927.251702	46.330356
3262.550082	427850.920977	46.335361
3258.829966	423781.465941	46.340365
3255.159472	419699.675103	46.345370
3251.302035	415628.349002	46.350375
3247.439303	411554.299598	46.355380
3243.768011	407458.384731	46.360385
3239.767867	403380.528938	46.365389
3236.029876	399284.709716	46.370394
3232.320749	395191.226692	46.375399
3228.333412	391108.484189	46.380404
3224.648610	387006.466897	46.385409
3220.587276	382925.154866	46.390413
3216.541994	378826.221018	46.395418
3212.795597	374744.437657	46.400423
3208.875687	370645.551096	46.405428
3205.132313	366559.346330	46.410433
3200.844228	362473.831128	46.415437
3197.087747	358395.128071	46.420442
3193.193132	354306.957926	46.425447
3189.086608	350233.720389	46.430452
3185.455901	346156.672283	46.435457
3181.120771	342089.535990	46.440461
3177.315237	338013.244327	46.445466
3173.178322	333950.019304	46.450471
3169.243691	329879.761445	46.455476
3165.689326	325817.219840	46.460481
3161.078564	321777.999297	46.465485
3157.294872	317716.012233	46.470490
3153.253641	313682.367335	46.475495
3148.970679	309648.593059	46.480500
3144.951762	305622.846089	46.485505
3140.810622	301614.730245	46.490509
3136.719423	297586.778464	46.495514
3132.775228	293599.339022	46.500519
3128.936985	289598.274056	46.505524
3124.838060	285615.108852	46.510529
3120.527624	281639.309121	46.515533
3116.637248	277665.540405	46.520538
3112.536605	273696.927292	46.525543
3108.374889	269759.718106	46.530548
3104.404410	265811.228296	46.535553
3100.297489	261873.989630	46.540557
3096.248776	257938.027011	46.545562
3092.061441	254024.933925	46.550567
3087.601807	250131.716207	46.555572
3083.804664	246225.431217	46.560577
3079.919477	242343.425662	46.565581
3075.610504	238464.808862	46.570586
3071.558219	234601.044498	46.575591
3067.450376	230745.703443	46.580596
3063.360077	226898.430535	46.585601
3059.224517	223063.985772	46.590605
3055.392907	219247.493249	46.595610
3051.128126	215434.750855	46.600615
3046.811239	211643.277318	46.605620
3043.360898	207760.040766	46.610625
3038.862742	203989.501813	46.615629
3034.877627	200214.765084	46.620634
3030.877713	196449.448783	46.625639
3026.620289	192708.266469	46.630644
3022.198200	188963.378305	46.635649
3018.204901	185250.815856	46.640653
3014.178424	181532.613998	46.645658
3010.286594	177846.053004	46.650663
3005.698392	174158.271804	46.655668
3001.583494	170475.591123	46.660673
2997.371575	166832.348567	46.665677
2993.692274	163177.206450	46.670682
2989.229908	159549.787296	46.675687
2985.157726	155944.268255	46.680692
2980.993567	152342.117438	46.685697
2976.498037	148764.060238	46.690701
2972.660139	145177.427881	46.695706
2968.852091	141627.099941	46.700711
2964.244441	138088.527501	46.705716
2960.063435	134553.050679	46.710721
2955.872048	131045.330489	46.715725
2951.863708	127540.480950	46.720730
2947.872742	124054.777429	46.725735
2943.390191	120585.881347	46.730740
2939.698987	117128.707706	46.735745
2935.050619	113696.849510	46.740749
2930.694613	110269.997634	46.745754
2926.766318	106859.198203	46.750759
2922.701205	103474.108837	46.755764
2918.490029	100093.841212	46.760769
2913.955351	96750.660939	46.765773
2909.899060	93397.661599	46.770778
2905.674554	90084.853810	46.775783
2901.415263	86778.146837	46.780788
2897.328934	83491.575894	46.785793
2892.942097	80230.363179	46.790797
2888.658891	76977.102638	46.795802
2884.407436	73741.975170	46.800807
2879.668781	70549.531288	46.805812
2875.403535	67353.659874	46.810817
2870.991542	64200.908870	46.815821
2866.189030	61061.803496	46.820826
2861.445241	57953.567815	46.825831
2856.420191	54879.849561	46.830836
2851.484859	51841.826833	46.835841
2845.846776	48860.550902	46.840845
2837.763682	45980.457604	46.845850
2827.533520	43215.471924	46.850855
2817.421173	40544.127976	46.855860
2808.312313	37991.880377	46.860865
2798.487399	35562.641105	46.865869
2789.192404	33245.801028	46.870874
2780.677083	31056.222346	46.875879
2772.425927	29008.223540	46.880884
2764.335896	27053.930327	46.885889
2756.525575	25254.996218	46.890893
2748.768182	23562.400992	46.895898
2740.948057	21989.973913	46.900903
2732.241606	20548.362058	46.905908
2724.837537	19212.517751	46.910913
2716.892843	18005.706920	46.915917
2709.739331	16899.174154	46.920922
2702.763247	15907.907820	46.925927
2695.979760	14994.609981	46.930932
2689.585316	14172.927125	46.935937
2683.560953	13442.246817	46.940941
2678.391941	12773.056235	46.945946
2672.991682	12185.096034	46.950951
2667.957247	11649.505427	46.955956
2664.035767	11157.937785	46.960961
2659.698929	10709.187944	46.965965
2656.033093	10300.657694	46.970970
2652.199217	9925.643171	46.975975
2648.844941	9571.776218	46.980980
2645.818966	9236.430590	46.985985
2642.263677	8926.407041	46.990989
2638.973152	8612.420565	46.995994
2636.135670	8313.934966	47.000999
2633.049769	8024.024483	47.006004
2630.474772	7736.397844	47.011009
2627.485537	7455.876467	47.016013
2624.161926	7173.414074	47.021018
2621.604227	6890.422806	47.026023
2618.337450	6618.790012	47.031028
2615.895916	6327.604501	47.036033
2612.483314	6048.224910	47.041037
2609.858878	5759.405545	47.046042
2606.905287	5461.900640	47.051047
2603.790916	5177.528330	47.056052
2601.094005	4874.904628	47.061057
2597.903500	4577.853420	47.066061
2594.924871	4266.015025	47.071066
2591.551722	3960.641710	47.076071
2588.327970	3660.516674	47.081076
2585.139255	3336.731598	47.086081
2581.556634	3035.216344	47.091085
2578.595173	2715.714528	47.096090
2574.858434	2402.418638	47.101095
2571.390673	2096.623179	47.106100
2567.946887	1784.992220	47.111105
2564.028687	1478.411291	47.116109
2560.261980	1178.436543	47.121114
2556.361605	895.750220	47.126119
2552.468298	622.418923	47.131124
2548.327206	344.214781	47.136129
2542.719023	138.683512	47.141133
2528.689445	190.319193	47.146138
2518.990549	182.631654	47.151143
2513.744197	191.282715	47.156148
2511.558264	178.642384	47.161153
2509.728291	182.584422	47.166157
2508.467027	189.254955	47.171162
2507.018218	191.997796	47.176167
2504.028449	182.665550	47.181172
2500.923130	181.392619	47.186177
2497.207462	189.125612	47.191181
2494.035907	184.713671	47.196186
2490.774630	181.966701	47.201191
2487.350188	194.255781	47.206196
2483.826516	179.225263	47.211201
2480.440093	191.275405	47.216205
2477.439109	183.539341	47.221210
2474.487652	171.695170	47.226215
2470.824745	181.253350	47.231220
2467.620510	176.095550	47.236225
2463.942138	183.293930	47.241229
2460.906520	174.909219	47.246234
2457.461593	175.816542	47.251239
2453.941545	180.274973	47.256244
2450.477324	175.304552	47.261249
2447.119847	182.135216	47.266253
2443.849854	176.012439	47.271258
2440.854530	171.596707	47.276263
2437.085167	171.554323	47.281268
2433.714134	176.210767	47.286273
2430.564105	181.286194	47.291277
2427.212400	170.759658	47.296282
2423.812747	175.571995	47.301287
2419.317620	171.997059	47.306292
2416.404980	166.678087	47.311297
2412.996393	165.326610	47.316301
2410.092259	172.687698	47.321306
2406.250980	163.705080	47.326311
2402.271309	174.214474	47.331316
2399.196096	166.620576	47.336321
2395.520160	171.505772	47.341325
2392.036508	168.711910	47.346330
2388.877318	166.384678	47.351335
2385.625483	177.511196	47.356340
2382.619862	161.289765	47.361345
2379.157651	171.941283	47.366349
2375.305007	160.904288	47.371354
2372.310827	169.120927	47.376359
2368.429895	175.743421	47.381364
2365.053623	172.882320	47.386369
2361.389921	179.909620	47.391373
2357.615530	167.321452	47.396378
2354.636527	172.392170	47.401383
2350.872183	175.376612	47.406388
2347.280454	168.538581	47.411393
2344.163515	168.805540	47.416397
2340.375210	164.633864	47.421402
2337.055404	167.860275	47.426407
2333.616019	163.244808	47.431412
2330.411315	168.011204	47.436417
2327.021335	164.624906	47.441421
2323.465989	165.820512	47.446426
2319.846931	163.561551	47.451431
2316.177828	172.990802	47.456436
2312.762075	161.549612	47.461441
2309.164629	165.696092	47.466445
2305.698098	166.903886	47.471450
2302.660407	158.989307	47.476455
2298.896808	166.998718	47.481460
2295.845733	163.715151	47.486465
2292.222156	161.871568	47.491469
2288.206613	158.472544	47.496474
2284.834027	165.204165	47.501479
2281.637786	163.913235	47.506484
2278.053819	153.114565	47.511489
2274.684695	166.930307	47.516493
2271.439178	157.971602	47.521498
2268.068644	143.851216	47.526503
2264.293119	168.236072	47.531508
2260.765686	152.364151	47.536513
2256.755416	161.130263	47.541517
2253.189112	156.446025	47.546522
2250.139666	155.950825	47.551527
2246.316094	162.929800	47.556532
2243.686804	155.906903	47.561537
2239.793502	160.722714	47.566541
2236.290091	160.395029	47.571546
2233.077342	157.917887	47.576551
2229.315055	163.393093	47.581556
2225.770660	156.595502	47.586561
2222.285999	163.356322	47.591565
2218.691200	163.097416	47.596570
2215.470995	152.929030	47.601575
2211.656191	155.785344	47.606580
2208.329574	151.850332	47.611585
2204.883647	161.509799	47.616589
2201.514146	164.794823	47.621594
2198.010106	154.015387	47.626599
2194.172822	159.778683	47.631604
2190.822508	146.050095	47.636609
2187.337803	156.171826	47.641613
2183.742435	154.118239	47.646618
2180.823355	151.627968	47.651623
2177.012070	159.283808	47.656628
2173.413601	158.310383	47.661633
2170.195294	150.336529	47.666637
2166.356106	155.446374	47.671642
2162.776669	149.233419	47.676647
2159.015234	159.206486	47.681652
2156.326431	153.639771	47.686657
2152.453983	157.110888	47.691661
2148.843511	148.246094	47.696666
2145.656199	148.036583	47.701671
2141.837223	152.310138	47.706676
2138.616894	155.019402	47.711681
2135.465592	155.482994	47.716685
2131.637354	158.426049	47.721690
2128.185488	147.424736	47.726695
2124.173519	162.521866	47.731700
2121.029730	152.820469	47.736705
2117.665551	151.395367	47.741709
2114.022428	154.272147	47.746714
2110.887140	148.684865	47.751719
2107.312722	153.339577	47.756724
2103.676521	146.725383	47.761729
2099.996724	147.193391	47.766733
2096.551324	155.496522	47.771738
2092.960231	148.984212	47.776743
2089.189161	159.895488	47.781748
2086.089699	152.706029	47.786753
2082.687712	150.048499	47.791757
2079.281941	156.411175	47.796762
2075.915058	155.968311	47.801767
2071.954815	154.884996	47.806772
2068.896195	152.855143	47.811777
2065.109280	149.185302	47.816781
2061.528839	158.607568	47.821786
2058.086257	148.713234	47.826791
2054.717883	158.102455	47.831796
2051.167563	150.632074	47.836801
2047.801461	148.993424	47.841805
2044.113697	153.944358	47.846810
2040.832125	151.429776	47.851815
2036.845198	142.916157	47.856820
2033.868350	146.991511	47.861825
2030.314360	149.566305	47.866829
2026.473839	143.650755	47.871834
2023.223869	144.766936	47.876839
2019.446319	147.148760	47.881844
2016.277878	138.521889	47.886849
2013.005609	149.481861	47.891853
2009.291686	149.277715	47.896858
2005.652451	142.588524	47.901863
2002.056227	155.797208	47.906868
1998.573317	143.483502	47.911873
1994.864086	145.192186	47.916877
1991.457207	147.948535	47.921882
1988.120259	141.586153	47.926887
1984.959586	144.379198	47.931892
1981.602290	143.785236	47.936897
1977.775848	146.081628	47.941901
1974.432856	140.892841	47.946906
1971.122987	145.497242	47.951911
1966.938430	145.160498	47.956916
1963.913620	138.341840	47.961921
1960.112309	140.790189	47.966925
1956.612719	148.391738	47.971930
1952.861963	146.561926	47.976935
1949.671167	150.529399	47.981940
1946.262629	149.695278	47.986945
1942.721095	148.591460	47.991949
1939.285519	156.943981	47.996954
1935.747965	136.891052	48.001959
1932.262888	145.489739	48.006964
1929.017160	143.611458	48.011969
1925.194079	140.592020	48.016973
1921.765959	138.213821	48.021978
1918.186429	137.028877	48.026983
1914.435877	148.321289	48.031988
1911.224503	137.073039	48.036993
1907.543414	146.971033	48.041997
1904.262247	148.027522	48.047002
1901.015593	142.469444	48.052007
1897.337669	143.244356	48.057012
1893.763734	138.153375	48.062017
1890.261221	142.718607	48.067021
1886.650355	150.942834	48.072026
1883.466974	143.239903	48.077031
1879.745609	143.397230	48.082036
1876.140889	142.173262	48.087041
1872.416617	141.239005	48.092045
1869.170880	146.810098	48.097050
1865.802389	142.641504	48.102055
1862.054908	147.224331	48.107060
1858.406348	145.118016	48.112065
1855.161343	148.803231	48.117069
1851.951258	144.744249	48.122074
1848.579772	140.488150	48.127079
1844.460153	143.412264	48.132084
1841.315022	136.393142	48.137089
1837.967251	138.265030	48.142093
1834.406935	146.610197	48.147098
1830.575839	133.522973	48.152103
1827.123843	138.959636	48.157108
1824.056932	132.534226	48.162113
1820.390068	132.374749	48.167117
1816.758404	133.584513	48.172122
1813.395194	119.676453	48.177127
1809.610655	139.921065	48.182132
1806.117558	130.726770	48.187137
1802.618759	140.603201	48.192141
1798.965758	144.799864	48.197146
1796.040302	139.978156	48.202151
1792.398006	142.456607	48.207156
1789.061152	132.480905	48.212161
1785.221304	146.965891	48.217165
1781.662814	145.887098	48.222170
1777.815068	131.991221	48.227175
1774.222392	150.901344	48.232180
1771.548626	137.921942	48.237185
1767.679073	134.761917	48.242189
1764.204744	138.684190	48.247194
1760.822614	131.558648	48.252199
1757.234587	140.339625	48.257204
1753.814542	134.671380	48.262209
1750.164422	133.581505	48.267213
1746.289036	140.007570	48.272218
1743.421868	136.127044	48.277223
1739.709983	138.455411	48.282228
1736.383205	128.407640	48.287233
1732.788487	134.280184	48.292237
1729.211741	135.755833	48.297242
1725.790773	134.823285	48.302247
1722.248988	137.310046	48.307252
1718.718196	139.074118	48.312257
1715.072484	137.711807	48.317261
1711.497095	137.294378	48.322266
1708.264014	131.449644	48.327271
1704.744314	133.570653	48.332276
1701.331115	130.718123	48.337281
1697.422042	134.053161	48.342285
1693.635378	128.527632	48.347290
1690.799391	130.006228	48.352295
1687.224346	138.780765	48.357300
1683.927007	129.913779	48.362305
1680.539936	136.988177	48.367309
1676.790275	135.438630	48.372314
1673.377624	138.859206	48.377319
1669.150734	131.190921	48.382324
1666.233725	129.383429	48.387329
1662.752713	127.834893	48.392333
1658.734141	129.584290	48.397338
1655.547818	130.545751	48.402343
1651.932086	132.761996	48.407348
1648.702339	124.599618	48.412353
1645.522842	130.882158	48.417357
1641.906822	130.451171	48.422362
1638.672711	122.882720	48.427367
1634.245404	132.351644	48.432372
1630.798549	136.649148	48.437377
1627.708794	133.933264	48.442381
1624.006640	135.609883	48.447386
1621.066385	130.220633	48.452391
1617.037505	136.089024	48.457396
1613.623346	127.775987	48.462401
1610.222012	132.209250	48.467405
1606.337303	127.913033	48.472410
1602.938763	119.373451	48.477415
1599.889756	129.324472	48.482420
1596.572903	128.532291	48.487425
1592.751358	126.134498	48.492429
1588.929197	129.828821	48.497434
1585.771312	124.736243	48.502439
1582.260201	127.734074	48.507444
1578.602768	114.474355	48.512449
1575.160343	124.903228	48.517453
1571.435343	125.027656	48.522458
1568.196048	124.965656	48.527463
1564.306844	123.042811	48.532468
1561.142039	126.589256	48.537473
1557.724555	123.060677	48.542477
1554.195938	129.110879	48.547482
1551.006569	128.887901	48.552487
1546.750738	131.847601	48.557492
1543.630159	121.183180	48.562497
1539.941358	125.172821	48.567501
1536.389671	127.505654	48.572506
1533.150454	124.126421	48.577511
1529.317242	127.095231	48.582516
1525.541993	124.620973	48.587521
1522.309406	130.061837	48.592525
1519.105721	127.729143	48.597530
1515.613073	120.139183	48.602535
1511.830226	120.347615	48.607540
1508.936317	119.599662	48.612545
1505.419202	120.218257	48.617549
1501.449492	123.907826	48.622554
1498.109520	122.052731	48.627559
1494.383825	126.239132	48.632564
1490.852394	117.926441	48.637569
1487.772445	126.265062	48.642573
1483.733963	120.486317	48.647578
1480.558131	120.244377	48.652583
1477.060311	125.730288	48.657588
1473.794461	123.039670	48.662593
1470.113244	126.477539	48.667597
1466.729357	123.382356	48.672602
1463.192203	117.916832	48.677607
1459.385831	123.340478	48.682612
1455.995894	123.917370	48.687617
1452.403432	119.462877	48.692621
1448.589360	123.531110	48.697626
1445.663413	123.136793	48.702631
1441.718659	135.055204	48.707636
1438.490425	121.276322	48.712641
1435.199419	123.297174	48.717645
1431.230844	128.171427	48.722650
1428.120758	121.108151	48.727655
1424.352311	126.476025	48.732660
1420.919856	126.369092	48.737665
1417.582308	133.047707	48.742669
1414.429820	119.654159	48.747674
1410.373074	121.539134	48.752679
1407.092536	134.081682	48.757684
1403.760850	113.749194	48.762689
1399.932174	119.284712	48.767693
1395.902736	119.336264	48.772698
1393.016071	119.331347	48.777703
1389.234513	131.106192	48.782708
1386.397915	122.062259	48.787713
1382.997718	117.245703	48.792717
1379.047787	126.206136	48.797722
1375.655037	126.014331	48.802727
1371.487161	134.115282	48.807732
1368.397374	122.658336	48.812737
1365.312873	125.568641	48.817741
1361.394690	131.206013	48.822746
1357.863118	119.299751	48.827751
1354.551901	121.661840	48.832756
1350.943162	127.236821	48.837761
1347.431549	127.416537	48.842765
1343.835829	128.291367	48.847770
1340.427592	112.251641	48.852775
1336.488953	116.870006	48.857780
1333.694549	125.078436	48.862785
1330.276846	119.247937	48.867789
1326.359364	122.889746	48.872794
1322.940438	120.170868	48.877799
1319.136106	116.218606	48.882804
1315.963877	124.016681	48.887809
1312.348451	115.551675	48.892813
1308.841892	124.026040	48.897818
1305.561738	118.837059	48.902823
1301.731143	121.441926	48.907828
1298.434733	118.551259	48.912833
1294.898680	118.618430	48.917837
1291.161829	119.533798	48.922842
1287.850354	115.948242	48.927847
1284.450486	121.514790	48.932852
1281.392553	115.887315	48.937857
1277.464307	116.058603	48.942861
1273.679009	122.546304	48.947866
1270.355956	107.709344	48.952871
1266.696219	119.431371	48.957876
1263.234474	115.179207	48.962881
1259.967626	119.335713	48.967885
1256.170976	116.233548	48.972890
1253.142470	117.031648	48.977895
1249.340701	118.768048	48.982900
1245.692399	108.103892	48.987905
1242.195543	114.876046	48.992909
1238.742140	117.527930	48.997914
1235.445585	123.535648	49.002919
1231.998666	118.973607	49.007924
1228.719625	121.155427	49.012929
1225.126210	124.085428	49.017933
1220.926797	120.529107	49.022938
1217.384814	121.693524	49.027943
1214.017842	126.095132	49.032948
1210.874275	115.406363	49.037953
1207.482363	122.074169	49.042957
1203.851061	127.324422	49.047962
1200.703842	116.571341	49.052967
1196.501633	118.687753	49.057972
1193.155083	120.890430	49.062977
1189.765376	112.506223	49.067981
1186.340802	112.981096	49.072986
1183.079448	113.197906	49.077991
1179.150418	124.992737	49.082996
1175.953438	120.020989	49.088001
1172.152031	119.923542	49.093005
1168.901161	117.755393	49.098010
1165.464973	107.812831	49.103015
1161.654085	120.250006	49.108020
1158.412094	116.496375	49.113025
1154.819355	108.571029	49.118029
1150.916368	114.574281	49.123034
1147.641849	114.577998	49.128039
1144.288818	115.772207	49.133044
1140.842690	119.120150	49.138049
1137.332668	120.335584	49.143053
1133.938044	125.035457	49.148058
1130.158423	108.322256	49.153063
1126.514706	123.037299	49.158068
1123.150521	116.174140	49.163073
1119.796343	114.984731	49.168077
1115.927438	122.197379	49.173082
1112.691078	107.079428	49.178087
1109.000562	113.106585	49.183092
1105.776747	109.394589	49.188097
1102.378824	109.316327	49.193101
1098.673886	119.032912	49.198106
1095.114101	115.977168	49.203111
1091.649523	114.327297	49.208116
1087.977887	106.394928	49.213121
1085.105096	110.753388	49.218125
1081.342926	112.257032	49.223130
1078.097263	101.022658	49.228135
1074.228621	115.483850	49.233140
1070.643432	103.205275	49.238145
1067.208161	108.824394	49.243149
1063.593633	112.847897	49.248154
1060.166948	108.396910	49.253159
1056.718643	111.812959	49.258164
1053.160173	98.640789	49.263169
1049.799082	107.764184	49.268173
1045.787363	120.025277	49.273178
1042.900824	108.726805	49.278183
1039.120496	113.793434	49.283188
1035.708777	115.023869	49.288193
1032.275948	109.933170	49.293197
1028.496403	108.372138	49.298202
1025.292546	107.011717	49.303207
1021.635439	107.032420	49.308212
1018.013745	111.515159	49.313217
1014.445720	114.004021	49.318221
1011.092637	119.496321	49.323226
1007.925726	116.297533	49.328231
1004.199268	111.726456	49.333236
1000.466951	105.387825	49.338241
997.205140	104.728869	49.343245
993.529070	102.714249	49.348250
990.407160	107.153429	49.353255
986.704061	108.394200	49.358260
983.201012	114.598048	49.363265
979.818610	105.975418	49.368269
975.979641	115.030091	49.373274
972.554705	116.769716	49.378279
968.896965	112.818978	49.383284
965.384911	111.678095	49.388289
962.044363	113.162233	49.393293
958.513903	121.965013	49.398298
955.122153	107.344928	49.403303
951.583144	116.141230	49.408308
948.132543	110.747273	49.413313
944.868573	112.900554	49.418317
941.055459	110.433062	49.423322
937.560944	104.436216	49.428327
933.856309	119.322285	49.433332
930.566884	105.037349	49.438337
927.464061	112.759257	49.443341
923.677867	108.133997	49.448346
920.074257	109.780667	49.453351
916.322741	116.445589	49.458356
912.887843	115.928198	49.463361
909.540620	111.129508	49.468365
905.775359	111.502481	49.473370
902.264854	103.981718	49.478375
898.921492	108.895868	49.483380
895.525202	112.212461	49.488385
892.074486	110.425872	49.493389
888.367318	118.396160	49.498394
885.578472	105.565125	49.503399
881.703503	106.449407	49.508404
878.078015	103.534362	49.513409
874.533675	112.478613	49.518413
870.779264	111.675869	49.523418
867.572283	116.827180	49.528423
864.256429	113.168084	49.533428
860.601622	102.087606	49.538433
857.015115	104.180435	49.543437
853.092934	110.935794	49.548442
850.082975	104.106234	49.553447
846.390359	112.396590	49.558452
842.948442	110.620820	49.563457
839.639681	106.873547	49.568461
835.941991	110.984585	49.573466
832.659311	101.947365	49.578471
829.335820	106.046042	49.583476
825.551057	113.696107	49.588481
821.805757	109.506010	49.593485
818.019074	109.719403	49.598490
815.152728	101.905682	49.603495
811.488544	108.833493	49.608500
807.907917	106.107041	49.613505
804.559662	111.688273	49.618509
800.893071	109.278957	49.623514
797.516615	105.156532	49.628519
793.804784	105.403544	49.633524
790.754771	108.174723	49.638529
787.257001	104.106908	49.643533
783.389357	109.219954	49.648538
779.802341	106.776575	49.653543
776.410428	105.671421	49.658548
772.864540	103.866731	49.663553
769.235461	109.005247	49.668557
765.753407	107.929813	49.673562
762.446256	97.697493	49.678567
758.876529	102.921313	49.683572
755.349675	105.704501	49.688577
751.931954	106.881284	49.693581
748.136776	116.001310	49.698586
744.851443	105.303230	49.703591
741.282395	112.930304	49.708596
737.567515	97.307942	49.713601
734.528059	97.440219	49.718605
730.747075	103.914399	49.723610
727.483919	97.167079	49.728615
724.058223	107.565112	49.733620
720.278372	107.372330	49.738625
716.792974	104.663353	49.743629
713.272021	103.161443	49.748634
709.758406	98.510032	49.753639
706.625655	100.874433	49.758644
703.004978	98.253167	49.763649
699.541904	105.388736	49.768653
695.379041	100.779036	49.773658
692.358429	98.172761	49.778663
688.757834	118.177832	49.783668
685.499093	105.131057	49.788673
682.237828	104.340030	49.793677
678.294334	116.449219	49.798682
675.134588	108.935742	49.803687
671.274410	116.281484	49.808692
667.810951	111.162607	49.813697
664.442046	101.749859	49.818701
660.578591	109.768668	49.823706
657.286461	107.706795	49.828711
653.465531	108.776512	49.833716
649.960131	107.456983	49.838721
646.774234	104.432503	49.843725
643.287346	108.458299	49.848730
639.739423	104.860868	49.853735
636.559469	100.010061	49.858740
633.347642	98.329395	49.863745
629.330808	100.273971	49.868749
625.469842	107.947256	49.873754
622.126810	96.488833	49.878759
618.432936	104.039952	49.883764
615.124708	102.412348	49.888769
612.046395	96.530244	49.893773
608.355853	105.129261	49.898778
604.947185	102.250208	49.903783
601.081557	102.421400	49.908788
597.439560	98.248553	49.913793
594.333719	97.847267	49.918797
590.874002	104.131842	49.923802
587.725617	102.974307	49.928807
584.091417	109.211787	49.933812
580.130458	110.922989	49.938817
576.670994	105.233823	49.943821
573.230368	101.557718	49.948826
569.579692	101.004473	49.953831
566.093155	111.494576	49.958836
562.899146	101.140301	49.963841
559.390347	102.294414	49.968845
555.221955	106.186969	49.973850
552.258544	99.289748	49.978855
548.562780	96.734913	49.983860
545.039271	93.056762	49.988865
541.997332	106.699145	49.993869
538.121751	102.446009	49.998874
535.004398	105.555881	50.003879
531.015608	104.030304	50.008884
527.450911	102.255373	50.013889
524.014499	103.611052	50.018893
520.678363	100.856621	50.023898
517.537141	104.720525	50.028903
513.443650	109.282319	50.033908
509.875720	106.705178	50.038913
506.807671	101.407934	50.043917
503.413098	102.150689	50.048922
499.701668	94.476857	50.053927
496.074508	100.855120	50.058932
492.735746	106.903275	50.063937
489.451872	100.527607	50.068941
485.821288	104.410356	50.073946
482.449006	99.395545	50.078951
478.193806	107.400790	50.083956
475.121712	102.038527	50.088961
471.674194	106.261784	50.093965
467.688880	111.455739	50.098970
464.710582	99.921898	50.103975
461.426598	101.088611	50.108980
457.805628	102.348986	50.113985
454.181054	93.650073	50.118989
450.335107	109.304986	50.123994
446.765836	102.731495	50.128999
443.569443	105.905028	50.134004
440.358041	103.884034	50.139009
436.619306	97.363465	50.144013
433.166234	109.407461	50.149018
429.732523	98.465447	50.154023
426.182074	94.927228	50.159028
422.381209	107.911074	50.164033
419.056434	93.805327	50.169037
415.301391	94.602483	50.174042
412.502348	97.534053	50.179047
408.496002	95.518161	50.184052
405.116204	97.622920	50.189057
401.677837	90.583412	50.194061
397.406235	101.002279	50.199066
394.579256	93.549204	50.204071
391.495917	100.921893	50.209076
387.939322	93.323576	50.214081
383.859954	99.077219	50.219085
380.492412	110.080164	50.224090
377.530469	93.986440	50.229095
373.428529	97.015282	50.234100
369.963851	90.783111	50.239105
366.644718	91.919798	50.244109
362.604266	97.741216	50.249114
359.332102	87.633704	50.254119
356.073273	96.792134	50.259124
352.417773	89.544308	50.264129
349.058220	91.616158	50.269133
345.518712	102.196478	50.274138
342.079876	87.273582	50.279143
338.289763	94.941680	50.284148
334.760984	97.604154	50.289153
331.534993	92.602750	50.294157
327.703770	97.296333	50.299162
324.601289	97.081758	50.304167
320.842539	91.261994	50.309172
317.585212	96.370108	50.314177
314.327693	91.462540	50.319181
310.420798	95.696836	50.324186
307.338985	92.484104	50.329191
303.456102	98.023155	50.334196
299.943306	92.435808	50.339201
296.595061	99.412549	50.344205
292.748224	95.825827	50.349210
289.428813	96.608206	50.354215
285.959684	92.015906	50.359220
282.520437	97.132451	50.364225
279.020991	95.170118	50.369229
275.353379	94.050025	50.374234
272.005660	89.279575	50.379239
268.503081	92.869576	50.384244
264.769979	98.210407	50.389249
261.585328	93.044744	50.394253
257.896069	105.293122	50.399258
254.609432	97.435337	50.404263
250.825757	95.079629	50.409268
247.258641	97.293662	50.414273
243.967538	92.514256	50.419277
240.236538	105.559684	50.424282
237.138690	89.693024	50.429287
233.363069	97.314803	50.434292
229.734778	96.003338	50.439297
226.671198	90.722545	50.444301
222.695147	98.650823	50.449306
219.447574	89.571617	50.454311
216.188194	92.238129	50.459316
212.417125	103.739556	50.464321
208.779356	86.118813	50.469325
204.968132	98.737882	50.474330
201.810673	100.599773	50.479335
198.413741	101.419132	50.484340
195.169514	102.683657	50.489345
191.705254	88.339948	50.494349
187.645583	95.316147	50.499354
184.635202	91.807915	50.504359
181.032153	97.635617	50.509364
177.242328	96.679897	50.514369
174.097747	96.276647	50.519373
170.334587	100.242179	50.524378
166.913442	91.371724	50.529383
163.319789	98.879368	50.534388
159.793806	94.304482	50.539393
156.134350	85.989327	50.544397
152.456343	99.507931	50.549402
149.113540	89.987132	50.554407
145.895317	91.963711	50.559412
142.138745	93.925628	50.564417
139.127978	98.138786	50.569421
135.342916	98.732770	50.574426
131.883278	91.066341	50.579431
128.397367	91.025113	50.584436
124.341324	92.071863	50.589441
121.167328	79.376456	50.594445
117.737945	95.998631	50.599450
114.289906	98.474653	50.604455
110.855086	91.256225	50.609460
107.375636	89.750910	50.614465
103.797517	88.892812	50.619469
100.426920	102.641757	50.624474
97.086830	92.961304	50.629479
93.291531	85.554929	50.634484
89.746975	95.982344	50.639489
86.700965	98.427339	50.644493
82.631118	102.401696	50.649498
79.392040	95.536080	50.654503
75.551351	92.303746	50.659508
71.939041	88.019107	50.664513
68.659511	96.413527	50.669517
64.900913	88.054885	50.674522
61.721909	83.679563	50.679527
58.554833	93.597728	50.684532
54.974601	89.832306	50.689537
51.771526	84.503711	50.694541
47.663395	89.915502	50.699546
44.203999	92.265981	50.704551
40.795783	94.823674	50.709556
36.691913	92.904408	50.714561
33.711684	92.343807	50.719565
30.225449	90.419753	50.724570
26.993770	88.560899	50.729575
23.337748	88.495437	50.734580
19.376233	96.135938	50.739585
15.856992	92.591725	50.744589
12.419136	106.419554	50.749594
9.367282	92.988869	50.754599
5.809322	93.475899	50.759604
2.466124	91.977314	50.764609