Tue Jun 21 11:10:46 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
0.744953	89.848321	0.000000
1.199311	93.977713	0.005005
1.117810	106.623960	0.010010
1.132927	102.943196	0.015014
1.394279	93.682109	0.020019
1.078894	90.001216	0.025024
0.956011	77.785942	0.030029
0.560413	71.009743	0.035034
0.237919	54.774709	0.040038
0.333551	53.411721	0.045043
-0.459913	55.715787	0.050048
-0.516421	40.400696	0.055053
-0.662467	41.873343	0.060058
-1.265496	38.139059	0.065062
-1.690593	31.646989	0.070067
-2.019396	31.368378	0.075072
-1.963218	38.972218	0.080077
-1.788748	24.250756	0.085082
-2.428843	36.100458	0.090086
-2.675400	19.218462	0.095091
-3.128172	25.904122	0.100096
-3.329847	27.621989	0.105101
-3.175301	20.078062	0.110106
-3.806349	22.061994	0.115110
-4.153881	18.850569	0.120115
-4.873953	27.261765	0.125120
-4.599843	28.375351	0.130125
-4.550832	21.272770	0.135130
-5.003095	23.360296	0.140134
-5.651210	16.061368	0.145139
-5.711367	21.298711	0.150144
-6.168503	9.683281	0.155149
-6.324786	11.974183	0.160154
-6.379260	22.661307	0.165158
-6.436691	15.140249	0.170163
-6.452937	15.838380	0.175168
-7.377673	8.739970	0.180173
-7.497644	12.255030	0.185178
-8.174693	12.062896	0.190182
-7.877370	15.702638	0.195187
-7.846965	16.659443	0.200192
-7.932503	23.285080	0.205197
-8.369187	19.356709	0.210202
-8.767955	27.642872	0.215206
-9.190304	20.211838	0.220211
-9.567066	16.248089	0.225216
-9.460764	26.831041	0.230221
-10.104415	14.394016	0.235226
-10.695754	19.840085	0.240230
-10.931648	13.984073	0.245235
-10.840221	13.869912	0.250240
-10.789499	16.315187	0.255245
-11.198703	11.982866	0.260250
-11.226692	19.290426	0.265254
-11.110870	10.974439	0.270259
-11.869990	25.551245	0.275264
-12.468055	18.829121	0.280269
-12.343055	13.861334	0.285274
-12.841902	26.167552	0.290278
-12.559443	10.776235	0.295283
-12.870398	16.080957	0.300288
-13.699643	18.369436	0.305293
-13.896565	12.586299	0.310298
-14.408652	19.078131	0.315302
-14.247699	11.397777	0.320307
-14.128412	11.887577	0.325312
-14.313242	11.109555	0.330317
-14.523497	11.149937	0.335322
-15.355192	13.328315	0.340326
-15.600943	17.624132	0.345331
-15.676803	16.941926	0.350336
-15.800287	6.935751	0.355341
-15.545535	9.872538	0.360346
-16.664012	18.082909	0.365350
-16.931290	7.707656	0.370355
-17.210449	22.043169	0.375360
-17.228955	6.037078	0.380365
-17.257536	16.480741	0.385370
-17.423180	17.631428	0.390374
-17.602624	18.922928	0.395379
-18.401820	23.329534	0.400384
-18.816657	17.974383	0.405389
-18.169706	32.810510	0.410394
-18.728253	20.567378	0.415398
-19.091036	14.947076	0.420403
-19.712799	21.484895	0.425408
-20.146883	24.208376	0.430413
-19.862183	12.432216	0.435418
-20.198086	20.728489	0.440422
-20.263021	9.566706	0.445427
-20.300282	17.505291	0.450432
-20.864452	17.307293	0.455437
-21.265363	14.825566	0.460442
-21.667437	21.775148	0.465446
-21.725199	13.168029	0.470451
-21.990877	21.788138	0.475456
-22.020206	20.582991	0.480461
-22.287405	20.964717	0.485466
-23.137494	16.243645	0.490470
-23.115427	16.408356	0.495475
-23.055791	23.874468	0.500480
-23.215786	19.032214	0.505485
-23.344280	16.307057	0.510490
-23.854824	23.379978	0.515494
-24.175827	21.572722	0.520499
-24.935905	20.434711	0.525504
-24.892860	21.724888	0.530509
-25.029866	19.756135	0.535514
-25.207774	28.637585	0.540518
-24.939444	16.411058	0.545523
-25.541689	23.761221	0.550528
-26.533473	21.597957	0.555533
-26.560371	11.599860	0.560538
-27.286482	21.956570	0.565542
-26.569007	9.446895	0.570547
-27.227486	14.782919	0.575552
-26.905743	19.074944	0.580557
-26.882445	13.539697	0.585562
-27.434015	28.792338	0.590566
-27.867290	18.817131	0.595571
-28.092799	21.225268	0.600576
-28.047571	16.330680	0.605581
-28.633881	16.488984	0.610586
-29.303122	10.026700	0.615590
-29.490845	14.614629	0.620595
-29.657258	12.157810	0.625600
-30.299538	12.777668	0.630605
-29.927629	14.856983	0.635610
-29.895901	22.428354	0.640614
-30.045320	16.588412	0.645619
-30.324349	23.410666	0.650624
-30.998839	20.119595	0.655629
-31.377127	22.057135	0.660634
-31.759806	25.856250	0.665638
-31.554074	16.441818	0.670643
-31.602667	12.798464	0.675648
-32.372785	12.544392	0.680653
-32.745243	13.640921	0.685658
-33.440674	14.935776	0.690662
-33.059301	13.209544	0.695667
-33.367242	21.670892	0.700672
-33.204522	16.718960	0.705677
-33.042384	14.884979	0.710682
-33.701090	19.643649	0.715686
-33.994385	14.542470	0.720691
-34.633212	8.038251	0.725696
-34.772236	28.310398	0.730701
-34.672219	17.718031	0.735706
-35.486158	21.899358	0.740710
-36.105605	12.238159	0.745715
-36.588842	14.418432	0.750720
-35.949505	21.515239	0.755725
-35.625554	15.727150	0.760730
-36.536100	22.196562	0.765734
-36.563473	15.158139	0.770739
-36.883297	17.672470	0.775744
-37.208080	17.156002	0.780749
-37.801506	13.767841	0.785754
-38.496205	20.693262	0.790758
-38.148014	16.508630	0.795763
-38.521409	19.364535	0.800768
-38.620124	22.973757	0.805773
-38.253677	26.911864	0.810778
-38.505720	27.052703	0.815782
-38.241820	22.465655	0.820787
-39.355572	18.951327	0.825792
-39.746244	18.914238	0.830797
-39.797744	15.205851	0.835802
-40.477599	24.572583	0.840806
-40.949039	12.730226	0.845811
-41.242677	19.670534	0.850816
-41.534688	24.784459	0.855821
-41.186790	21.353684	0.860826
-41.618450	28.154644	0.865830
-41.514042	24.642634	0.870835
-41.607985	22.943016	0.875840
-41.792757	24.997300	0.880845
-42.507363	21.215793	0.885850
-42.924080	23.271980	0.890854
-42.975336	16.638688	0.895859
-43.224894	19.413900	0.900864
-43.393719	18.396430	0.905869
-43.365249	22.274077	0.910874
-44.139648	27.309625	0.915878
-44.317374	19.332917	0.920883
-44.245413	26.642081	0.925888
-44.404508	26.857117	0.930893
-44.449129	14.005172	0.935898
-45.354473	21.610754	0.940902
-45.624228	15.057849	0.945907
-45.851278	25.267785	0.950912
-45.761214	20.162519	0.955917
-45.810904	22.021373	0.960922
-46.741365	21.688875	0.965926
-47.126362	12.121067	0.970931
-47.390886	17.773497	0.975936
-47.588970	14.130035	0.980941
-47.363303	20.806944	0.985946
-47.866051	21.928801	0.990950
-47.431322	21.414628	0.995955
-47.924363	20.288443	1.000960
-48.516456	21.964800	1.005965
-48.836483	19.707861	1.010970
-49.134981	19.656298	1.015974
-48.817139	25.001935	1.020979
-49.497861	20.083905	1.025984
-50.190884	25.820321	1.030989
-50.289421	11.919406	1.035994
-50.591422	21.332294	1.040998
-50.414252	19.379003	1.046003
-50.756752	25.621743	1.051008
-50.665886	23.130212	1.056013
-50.635616	22.043068	1.061018
-52.075643	26.461871	1.066022
-51.898387	12.237835	1.071027
-52.338392	25.015207	1.076032
-52.195874	20.294736	1.081037
-52.228113	17.119312	1.086042
-52.545918	24.286214	1.091046
-53.007890	15.401294	1.096051
-53.564965	16.758488	1.101056
-53.859396	17.585368	1.106061
-53.782220	8.679051	1.111066
-54.143469	18.421822	1.116070
-54.257219	15.754017	1.121075
-54.418760	20.008658	1.126080
-54.720641	18.388270	1.131085
-55.185239	13.492272	1.136090
-55.807282	20.653908	1.141094
-55.113050	17.942283	1.146099
-55.791853	16.223686	1.151104
-56.043085	21.245412	1.156109
-55.927179	16.910398	1.161114
-56.767266	26.043976	1.166118
-57.137623	19.885031	1.171123
-57.366054	16.238504	1.176128
-57.312224	25.453348	1.181133
-57.063332	21.838281	1.186138
-57.558065	30.664651	1.191142
-57.467441	17.673487	1.196147
-58.312247	17.676479	1.201152
-58.832916	23.957802	1.206157
-58.705052	16.834274	1.211162
-59.122137	14.079360	1.216166
-58.675547	13.758976	1.221171
-59.588658	24.623018	1.226176
-60.219888	23.685872	1.231181
-59.994389	12.703521	1.236186
-60.578143	15.225843	1.241190
-60.425835	23.454686	1.246195
-60.477205	26.266738	1.251200
-61.330360	24.567147	1.256205
-61.777755	22.383200	1.261210
-62.095061	16.681768	1.266214
-62.231261	13.218288	1.271219
-61.977280	12.743716	1.276224
-62.167003	12.751495	1.281229
-61.980801	7.636627	1.286234
-62.408165	18.551253	1.291238
-62.281582	6.976122	1.296243
-63.049137	12.316004	1.301248
-63.406670	11.984140	1.306253
-63.575415	17.583610	1.311258
-64.683716	13.732134	1.316262
-64.935044	16.361613	1.321267
-65.001085	11.377711	1.326272
-64.968654	17.872512	1.331277
-65.119889	9.402435	1.336282
-65.041145	11.211998	1.341286
-65.392737	2.204222	1.346291
-65.412611	9.366771	1.351296
-65.965968	16.972672	1.356301
-66.429251	5.658025	1.361306
-66.773301	20.686456	1.366310
-66.746474	17.782450	1.371315
-66.819124	18.341132	1.376320
-66.785015	18.141547	1.381325
-67.627812	17.725666	1.386330
-68.204028	15.575881	1.391334
-68.593791	15.220939	1.396339
-68.514215	11.613588	1.401344
-68.430859	13.460275	1.406349
-68.614580	14.606458	1.411354
-68.345726	11.706574	1.416358
-69.136627	11.892844	1.421363
-69.844905	21.697625	1.426368
-70.109640	22.293446	1.431373
-70.183509	11.604379	1.436378
-70.175707	24.430331	1.441382
-70.154466	19.767833	1.446387
-71.123723	19.645412	1.451392
-71.950495	19.898006	1.456397
-71.427693	10.424363	1.461402
-71.555634	28.000094	1.466406
-71.581167	14.030062	1.471411
-71.617942	19.330031	1.476416
-71.869539	13.120441	1.481421
-72.565468	8.386682	1.486426
-73.265271	13.677853	1.491430
-73.262813	8.725627	1.496435
-73.347126	18.015438	1.501440
-73.829603	20.801795	1.506445
-73.594817	16.483206	1.511450
-73.621265	20.511039	1.516454
-74.478347	20.389380	1.521459
-74.688781	12.827956	1.526464
-75.059952	19.144312	1.531469
-74.934821	15.186452	1.536474
-75.013620	19.636760	1.541478
-75.044993	16.751865	1.546483
-75.842253	22.148570	1.551488
-76.398939	18.878452	1.556493
-76.044216	8.831964	1.561498
-76.576290	22.253873	1.566502
-76.709743	17.521879	1.571507
-77.574728	16.942140	1.576512
-77.999907	19.812346	1.581517
-77.428754	12.434259	1.586522
-77.864660	24.530746	1.591526
-77.915461	19.142747	1.596531
-78.107063	19.787235	1.601536
-77.975615	12.962273	1.606541
-78.718146	16.270227	1.611546
-79.405617	19.205380	1.616550
-79.362607	18.610246	1.621555
-79.239393	14.357692	1.626560
-79.703599	27.176961	1.631565
-80.080945	14.117078	1.636570
-80.917325	22.286468	1.641574
-80.933226	11.933332	1.646579
-80.935440	14.698760	1.651584
-81.052543	18.416993	1.656589
-81.121176	13.857983	1.661594
-81.566818	21.873075	1.666598
-81.294112	11.829513	1.671603
-81.803172	19.472479	1.676608
-82.451038	21.508933	1.681613
-82.509817	18.310082	1.686618
-82.752592	25.908558	1.691622
-83.267658	14.550191	1.696627
-84.219963	22.394632	1.701632
-83.546626	13.476215	1.706637
-83.713766	14.756798	1.711642
-84.338235	28.307282	1.716646
-84.542610	17.014676	1.721651
-84.564892	21.760306	1.726656
-84.688858	13.523302	1.731661
-84.518540	9.761411	1.736666
-85.363012	22.878279	1.741670
-86.045962	19.644070	1.746675
-85.970671	25.711456	1.751680
-85.676897	23.339846	1.756685
-85.923500	10.235425	1.761690
-86.854953	20.685542	1.766694
-87.397453	10.348774	1.771699
-87.562696	15.149651	1.776704
-87.901442	23.162038	1.781709
-87.587668	16.993400	1.786714
-87.878969	22.748932	1.791718
-87.891810	17.980784	1.796723
-87.742792	15.825350	1.801728
-88.281964	17.698961	1.806733
-88.825020	7.573828	1.811738
-89.151540	21.660251	1.816742
-89.237189	20.210269	1.821747
-89.361324	17.025004	1.826752
-89.941830	28.514174	1.831757
-90.443838	15.610899	1.836762
-91.073332	19.245665	1.841766
-90.865260	13.206815	1.846771
-90.910351	18.337665	1.851776
-91.257637	22.690555	1.856781
-90.825844	15.918071	1.861786
-91.307529	16.940145	1.866790
-91.422614	12.822171	1.871795
-92.105682	14.593912	1.876800
-92.559679	19.663031	1.881805
-92.474674	11.007807	1.886810
-92.688156	16.403934	1.891814
-92.992821	4.732888	1.896819
-93.597897	16.738591	1.901824
-94.106228	17.903014	1.906829
-93.945362	8.967053	1.911834
-94.615670	15.373993	1.916838
-94.544154	10.867747	1.921843
-94.706875	8.663499	1.926848
-94.802671	14.287787	1.931853
-94.631494	1.863655	1.936858
-95.090142	28.042585	1.941862
-95.320577	4.515153	1.946867
-95.456799	15.817862	1.951872
-95.585103	16.083448	1.956877
-96.681960	8.943714	1.961882
-96.918502	18.307870	1.966886
-97.200888	5.469860	1.971891
-97.337525	11.015663	1.976896
-97.427965	15.872232	1.981901
-97.513202	10.611102	1.986906
-97.819239	13.807895	1.991910
-98.033829	9.075924	1.996915
-98.748482	5.419159	2.006912
-97.859877	7.689726	2.016909
-97.554297	7.842119	2.026906
-97.491431	9.264872	2.036902
-96.219869	11.089099	2.046899
-96.025486	9.916725	2.056896
-95.985038	11.730458	2.066893
-95.050937	13.845303	2.076890
-95.048376	10.063380	2.086886
-94.057519	12.536531	2.096883
-93.696073	10.561561	2.106880
-93.114753	13.470243	2.116877
-92.063352	7.696247	2.126874
-92.106755	14.713239	2.136870
-92.170129	20.969283	2.146867
-90.920432	21.764554	2.156864
-90.689255	18.258928	2.166861
-90.065967	15.480286	2.176858
-89.237538	13.374039	2.186854
-89.093663	25.101076	2.196851
-89.082902	16.889908	2.206848
-87.896964	13.584191	2.216845
-87.720255	16.179134	2.226842
-87.027334	15.687667	2.236838
-86.132970	14.763519	2.246835
-85.941184	17.223386	2.256832
-85.735333	12.444568	2.266829
-85.466853	18.951713	2.276826
-84.785154	15.009106	2.286822
-83.983260	11.570789	2.296819
-82.853517	8.712623	2.306816
-82.942623	3.740020	2.316813
-82.970253	10.522435	2.326810
-82.241031	12.626756	2.336806
-81.813603	18.495460	2.346803
-81.012580	21.515554	2.356800
-80.198302	15.651211	2.366797
-80.072095	17.380402	2.376794
-79.943534	13.943143	2.386790
-78.913660	14.363449	2.396787
-78.634077	13.339183	2.406784
-78.231392	18.650843	2.416781
-77.296541	15.942121	2.426778
-76.859291	14.623029	2.436774
-76.927663	19.489099	2.446771
-75.996812	15.493575	2.456768
-75.391602	15.240893	2.466765
-75.312244	18.234880	2.476762
-74.444391	16.634642	2.486758
-74.085582	22.874910	2.496755
-73.625615	19.453700	2.506752
-72.501781	21.495046	2.516749
-72.107854	24.107367	2.526746
-71.879254	13.031298	2.536742
-72.257800	14.816417	2.546739
-71.427294	15.132617	2.556736
-70.645675	15.963324	2.566733
-69.567515	11.115130	2.576730
-69.201094	16.073587	2.586726
-68.936774	12.932551	2.596723
-69.054656	17.005612	2.606720
-68.126168	13.138319	2.616717
-67.604120	15.789883	2.626714
-66.898411	18.757005	2.636710
-66.082776	21.495100	2.646707
-65.954525	19.183337	2.656704
-66.046024	25.818663	2.666701
-64.978468	17.570004	2.676698
-64.498786	17.260263	2.686694
-64.072083	14.699712	2.696691
-63.096639	15.534481	2.706688
-62.810872	14.135163	2.716685
-62.553362	11.411962	2.726682
-62.444351	11.706965	2.736678
-61.600089	16.202185	2.746675
-61.166446	15.933461	2.756672
-59.843325	16.818141	2.766669
-59.759236	18.412639	2.776666
-59.488291	17.409563	2.786662
-59.549143	19.507406	2.796659
-58.724490	14.074059	2.806656
-58.255404	23.766256	2.816653
-57.024796	21.238549	2.826650
-56.609904	24.126588	2.836646
-56.636753	18.845512	2.846643
-56.432284	18.773204	2.856640
-55.528761	17.969653	2.866637
-54.985005	20.417471	2.876634
-54.415937	18.741447	2.886630
-53.571403	14.889837	2.896627
-53.693405	17.512318	2.906624
-53.348463	19.241446	2.916621
-52.398330	15.656279	2.926618
-51.948516	12.672429	2.936614
-51.291669	20.359261	2.946611
-50.645962	19.657681	2.956608
-50.222954	21.148833	2.966605
-50.164778	14.671328	2.976602
-49.792113	16.631387	2.986598
-48.833112	15.313030	2.996595
-48.491742	19.271313	3.006592
-48.134386	19.160844	3.016589
-47.140444	22.816837	3.026586
-47.017113	14.545138	3.036582
-46.911750	17.503996	3.046579
-46.505653	14.563939	3.056576
-45.125365	23.692687	3.066573
-44.511260	18.127643	3.076570
-44.101483	22.415632	3.086566
-44.233543	18.514131	3.096563
-44.103467	19.539478	3.106560
-43.184348	21.438487	3.116557
-41.973996	20.015280	3.126554
-41.860629	17.250548	3.136550
-41.367021	20.250427	3.146547
-41.148100	14.623384	3.156544
-40.505061	15.784093	3.166541
-39.811989	10.877369	3.176538
-39.888968	12.446971	3.186534
-38.728446	14.583216	3.196531
-38.298469	14.519800	3.206528
-38.194479	17.966526	3.216525
-36.971392	12.979147	3.226522
-36.541159	9.333864	3.236518
-36.296191	13.197267	3.246515
-36.045149	14.574239	3.256512
-36.096648	21.363183	3.266509
-34.866652	17.127064	3.276506
-34.585775	19.049767	3.286502
-33.915247	12.828290	3.296499
-33.358792	22.373049	3.306496
-32.955978	14.218471	3.316493
-31.891655	15.341822	3.326490
-31.686149	16.623592	3.336486
-31.736460	13.611519	3.346483
-31.364224	19.161774	3.356480
-30.262982	14.910622	3.366477
-29.917899	10.420537	3.376474
-29.412833	13.389080	3.386470
-28.374367	11.174758	3.396467
-28.108291	16.344656	3.406464
-28.229461	18.639008	3.416461
-27.847454	13.876661	3.426458
-27.074680	20.734993	3.436454
-26.544264	12.180318	3.446451
-25.335774	17.599208	3.456448
-25.096012	15.618113	3.466445
-24.930043	14.429699	3.476442
-24.953805	9.581023	3.486438
-23.848287	9.151055	3.496435
-23.405216	12.338712	3.506432
-23.067053	14.514717	3.516429
-22.119580	14.897508	3.526426
-21.454665	18.533897	3.536422
-21.726025	16.111073	3.546419
-21.297641	21.085359	3.556416
-20.405085	16.706745	3.566413
-19.973557	11.804014	3.576410
-19.114801	12.897391	3.586406
-18.920173	15.006474	3.596403
-18.538629	13.535777	3.606400
-17.560065	18.677991	3.616397
-17.426642	20.742874	3.626394
-17.437996	23.006594	3.636390
-16.212813	17.948332	3.646387
-15.979265	21.881994	3.656384
-15.308661	23.014828	3.666381
-14.441298	17.822976	3.676378
-14.404923	15.597953	3.686374
-14.129889	15.227858	3.696371
-13.600388	21.559014	3.706368
-12.701901	18.814635	3.716365
-12.494179	22.211783	3.726362
-11.700318	14.824878	3.736358
-10.965790	17.995098	3.746355
-11.071688	19.207908	3.756352
-10.749280	23.855749	3.766349
-9.700320	21.592864	3.776346
-9.000396	18.014164	3.786342
-9.084838	14.231626	3.796339
-8.701734	19.710734	3.806336
-7.594405	16.376559	3.816333
-7.608268	16.682229	3.826330
-6.489276	18.405294	3.836326
-6.055757	17.897518	3.846323
-6.274736	19.261040	3.856320
-5.460693	20.696139	3.866317
-4.768595	22.921422	3.876314
-4.780760	27.692438	3.886310
-3.951915	38.386117	3.896307
-3.714003	41.493550	3.906304
-3.306797	49.507258	3.916301
-2.802374	57.410623	3.926298
-2.015887	74.703795	3.936294
-1.427121	87.928429	3.946291
-1.209866	93.541328	3.956288
-0.993374	97.751294	3.966285
-0.260892	108.891521	3.976282
0.000000	126.519232	3.981286
0.475291	129.606203	3.986291
0.336529	134.741160	3.991296
0.944224	135.986985	3.996301
1.049325	149.359539	4.001306
0.924437	136.348109	4.006310
1.119744	128.726536	4.011315
0.382880	134.106756	4.016320
1.116540	132.722373	4.021325
0.681453	141.039080	4.026330
0.968423	150.482591	4.031334
1.317271	145.424810	4.036339
0.899168	145.263991	4.041344
0.933901	132.634023	4.046349
0.733798	144.426144	4.051354
0.914090	149.008230	4.056358
1.259302	148.181109	4.061363
1.198982	155.899413	4.066368
1.142657	142.543326	4.071373
0.914925	138.356743	4.076378
0.856323	146.027199	4.081382
1.098610	150.311504	4.086387
0.993041	158.200299	4.091392
1.314951	162.001766	4.096397
1.061148	164.719886	4.101402
1.091678	160.055607	4.106406
1.345856	163.259908	4.111411
1.023901	158.030024	4.116416
1.179773	160.626434	4.121421
1.015234	162.632985	4.126426
1.033389	167.132601	4.131430
0.904383	168.029577	4.136435
0.786431	169.116334	4.141440
1.272273	160.055428	4.146445
1.086285	166.438858	4.151450
1.131129	167.249819	4.156454
1.354516	160.864618	4.161459
0.908879	167.588229	4.166464
1.209160	156.226348	4.171469
1.269261	165.237186	4.176474
1.566678	164.925326	4.181478
1.343993	159.162382	4.186483
1.082081	169.372466	4.191488
1.289564	162.478012	4.196493
0.935169	162.618433	4.201498
1.081448	171.121076	4.206502
1.351314	186.028480	4.211507
1.395613	187.665379	4.216512
1.840047	183.184946	4.221517
1.839121	182.400142	4.226522
1.752982	175.870235	4.231526
1.678409	168.112574	4.236531
1.399684	171.200285	4.241536
1.480462	162.945470	4.246541
1.431726	168.131244	4.251546
1.411347	171.575582	4.256550
1.480723	161.102246	4.261555
1.402134	166.459710	4.266560
1.436108	155.619082	4.271565
1.384078	167.073926	4.276570
1.387760	166.338483	4.281574
1.293303	172.410757	4.286579
1.444510	189.425613	4.291584
1.661278	179.328054	4.296589
1.607484	189.939799	4.301594
1.436680	180.987417	4.306598
1.836242	192.405193	4.311603
1.864678	196.984812	4.316608
2.000066	192.271586	4.321613
1.940225	189.674544	4.326618
1.750882	177.813361	4.331622
1.235232	174.612967	4.336627
1.785878	181.451630	4.341632
2.207520	175.714201	4.346637
1.715841	167.510170	4.351642
1.640227	164.526403	4.356646
1.703476	162.057577	4.361651
1.616636	175.124297	4.366656
2.162606	177.225333	4.371661
1.777630	178.638890	4.376666
1.645845	163.613397	4.381670
1.915764	170.773032	4.386675
1.614356	170.838966	4.391680
2.127449	176.735652	4.396685
1.620720	185.264737	4.401690
2.122021	189.214897	4.406694
2.015415	186.210605	4.411699
1.588317	183.378178	4.416704
1.628191	174.463138	4.421709
1.603759	198.429983	4.426714
2.017787	197.516872	4.431718
2.025368	192.152884	4.436723
1.971375	197.952855	4.441728
2.244346	188.983619	4.446733
2.065133	194.047939	4.451738
2.030155	198.200765	4.456742
1.821297	198.330308	4.461747
1.703144	199.400524	4.466752
2.149046	198.130089	4.471757
1.841694	199.852451	4.476762
1.906529	191.465283	4.481766
2.030102	196.663579	4.486771
1.512503	191.621975	4.491776
1.983502	191.631838	4.496781
1.937494	201.631945	4.501786
1.680493	193.854356	4.506790
2.195966	206.690731	4.511795
2.305418	219.863515	4.516800
2.381924	207.854094	4.521805
1.895254	203.565723	4.526810
2.398204	207.255527	4.531814
2.259676	200.208585	4.536819
2.008034	203.485996	4.541824
2.584300	212.414549	4.546829
1.893188	210.141077	4.551834
2.329210	211.696932	4.556838
2.539118	211.994921	4.561843
2.213594	207.694863	4.566848
2.160174	190.576456	4.571853
2.361157	201.839653	4.576858
2.316295	207.227462	4.581862
2.335106	205.300173	4.586867
2.299044	219.083926	4.591872
2.517761	212.425971	4.596877
2.085354	214.760454	4.601882
2.342038	219.922904	4.606886
2.418339	223.883063	4.611891
2.623357	233.507930	4.616896
2.507339	223.033875	4.621901
2.505039	212.508240	4.626906
2.270725	210.939785	4.631910
2.589177	213.592559	4.636915
2.477444	226.026841	4.641920
2.499824	219.649838	4.646925
2.033100	206.551096	4.651930
2.582681	222.037572	4.656934
2.746382	218.206671	4.661939
2.632492	237.743613	4.666944
2.951739	217.461157	4.671949
2.431235	211.065321	4.676954
2.179049	205.897869	4.681958
2.621340	216.172135	4.686963
2.353046	220.071150	4.691968
2.629350	220.432541	4.696973
2.407475	229.738554	4.701978
2.677633	222.795215	4.706982
2.542986	231.598578	4.711987
2.357334	227.244766	4.716992
2.725142	226.060472	4.721997
2.538049	229.960843	4.727002
2.483327	224.722207	4.732006
2.782004	218.350564	4.737011
2.306269	226.571827	4.742016
2.856545	227.904326	4.747021
2.686896	225.187129	4.752026
2.441946	222.157983	4.757030
2.700988	221.511678	4.762035
2.583139	224.997032	4.767040
2.465931	221.119503	4.772045
2.766953	236.760423	4.777050
2.847326	246.056062	4.782054
3.201664	241.953431	4.787059
2.687235	242.009844	4.792064
2.986505	236.657727	4.797069
2.527114	234.176173	4.802074
2.832259	243.569371	4.807078
3.204378	245.122195	4.812083
3.245456	242.371878	4.817088
3.012961	224.625169	4.822093
2.533494	231.789336	4.827098
2.828843	230.778658	4.832102
3.208385	237.702116	4.837107
2.745362	235.289243	4.842112
3.232374	242.999050	4.847117
3.142268	239.282002	4.852122
2.882536	228.289661	4.857126
3.249762	218.721280	4.862131
3.239813	232.566434	4.867136
3.015976	226.308146	4.872141
2.898355	231.683739	4.877146
2.714434	228.861949	4.882150
2.883948	234.119745	4.887155
2.949588	246.883232	4.892160
3.280980	247.508022	4.897165
3.163755	255.479309	4.902170
3.222130	252.088534	4.907174
3.425247	257.564553	4.912179
3.098910	256.410147	4.917184
3.436130	245.009721	4.922189
3.259863	231.867596	4.927194
2.789755	228.364633	4.932198
3.175319	240.544504	4.937203
3.558811	248.195087	4.942208
3.464911	243.835549	4.947213
2.959758	225.042526	4.952218
2.914414	226.046421	4.957222
3.205202	228.752914	4.962227
3.211493	244.196568	4.967232
3.498286	239.533836	4.972237
3.512948	251.244497	4.977242
3.389480	249.181118	4.982246
3.361837	236.467068	4.987251
3.078651	250.145148	4.992256
3.473658	244.183394	4.997261
3.390043	254.919115	5.002266
3.597053	256.414426	5.007270
3.487589	252.626777	5.012275
3.001331	255.376497	5.017280
3.479041	253.534043	5.022285
3.305335	240.984283	5.027290
3.156829	245.220844	5.032294
3.370429	241.524941	5.037299
3.033330	248.368156	5.042304
3.349549	248.334582	5.047309
3.554758	250.640648	5.052314
3.425936	251.256394	5.057318
3.382444	248.176518	5.062323
3.209189	254.119001	5.067328
3.535166	250.805079	5.072333
3.434296	259.561622	5.077338
3.452315	254.680540	5.082342
3.449524	248.412282	5.087347
3.294740	265.355936	5.092352
3.591581	275.510272	5.097357
3.875644	286.169739	5.102362
3.613599	270.690526	5.107366
3.649574	273.755946	5.112371
3.451490	280.247197	5.117376
3.577881	284.053246	5.122381
3.597993	284.628348	5.127386
3.725812	292.342798	5.132390
3.476528	284.055152	5.137395
3.398900	284.759315	5.142400
3.795536	278.567579	5.147405
3.638254	280.441517	5.152410
3.381130	289.783595	5.157414
3.618085	285.214944	5.162419
3.815925	293.893232	5.167424
3.964171	280.565313	5.172429
3.885607	283.007964	5.177434
3.800584	289.803932	5.182438
4.098381	283.170937	5.187443
3.895370	301.599480	5.192448
3.774443	284.820712	5.197453
3.770525	287.291654	5.202458
3.726882	294.986742	5.207462
4.040672	287.130179	5.212467
3.693727	294.189944	5.217472
4.146410	282.332088	5.222477
3.665982	294.782878	5.227482
3.963432	284.520929	5.232486
3.899001	285.682107	5.237491
3.531038	283.042731	5.242496
3.980668	282.523128	5.247501
3.719485	296.417044	5.252506
3.833402	291.959736	5.257510
4.083074	308.389301	5.262515
4.134655	307.302949	5.267520
4.757085	300.306177	5.272525
4.045400	301.387064	5.277530
3.807210	287.792984	5.282534
4.160842	287.319470	5.287539
4.019972	285.736324	5.292544
3.976975	280.948021	5.297549
4.072375	286.651260	5.302554
3.841473	283.106307	5.307558
4.364594	301.942288	5.312563
4.177841	300.530724	5.317568
4.256819	295.643483	5.322573
4.241382	300.227831	5.327578
4.137460	293.155974	5.332582
4.298529	298.748689	5.337587
4.108584	295.462565	5.342592
4.339621	292.512259	5.347597
3.958681	295.792155	5.352602
4.171571	301.162378	5.357606
4.476632	304.296122	5.362611
4.338383	312.484438	5.367616
4.574631	313.143535	5.372621
4.357932	301.498726	5.377626
4.370811	290.983350	5.382630
4.223016	289.346294	5.387635
4.021566	289.751670	5.392640
4.416007	300.310187	5.397645
4.344216	306.871903	5.402650
4.459956	314.034244	5.407654
4.636027	309.359239	5.412659
4.186135	319.960292	5.417664
4.701800	301.840571	5.422669
4.680842	310.315138	5.427674
4.098683	307.527900	5.432678
4.680818	304.699425	5.437683
4.358108	296.448006	5.442688
4.561818	297.832175	5.447693
4.660119	301.058567	5.452698
4.471211	298.118005	5.457702
4.397501	297.040560	5.462707
4.537535	313.732193	5.467712
4.790171	303.303206	5.472717
4.730281	296.945123	5.477722
4.327383	286.835451	5.482726
4.159822	289.583120	5.487731
4.681714	305.488869	5.492736
4.715529	300.002097	5.497741
4.581081	312.656096	5.502746
4.663537	304.416912	5.507750
4.517624	310.155382	5.512755
4.433017	317.599148	5.517760
4.408778	307.397753	5.522765
4.498491	322.996789	5.527770
4.363706	310.915319	5.532774
4.575847	306.236118	5.537779
4.682242	316.052799	5.542784
4.895762	311.521173	5.547789
4.755982	317.873530	5.552794
4.591001	315.112920	5.557798
4.965873	316.654837	5.562803
4.800593	312.428462	5.567808
4.517955	312.808999	5.572813
4.865492	310.387994	5.577818
4.799306	304.620986	5.582822
4.906072	308.444302	5.587827
4.746479	317.652042	5.592832
4.794339	304.306586	5.597837
4.654336	313.553902	5.602842
4.664419	314.304717	5.607846
4.784659	311.133779	5.612851
4.675237	331.568769	5.617856
5.231650	333.841557	5.622861
5.291956	326.566861	5.627866
4.908438	322.883973	5.632870
4.826743	315.049666	5.637875
4.808360	322.180149	5.642880
5.070255	320.093996	5.647885
4.685086	324.665968	5.652890
4.972549	337.207302	5.657894
5.064511	340.450341	5.662899
5.187485	348.477808	5.667904
5.488937	340.464603	5.672909
5.159605	334.575394	5.677914
4.905757	316.899407	5.682918
5.095187	311.798113	5.687923
4.835182	328.059109	5.692928
5.369914	337.297130	5.697933
5.282511	337.151406	5.702938
4.782037	332.673473	5.707942
5.307091	334.203943	5.712947
5.144076	361.059315	5.717952
5.278113	349.447759	5.722957
5.297624	333.357873	5.727962
5.223774	336.966011	5.732966
5.327261	327.861365	5.737971
5.158389	325.880482	5.742976
5.026413	322.964626	5.747981
5.034220	338.349711	5.752986
5.202778	342.503407	5.757990
5.316383	340.117581	5.762995
5.341017	352.697515	5.768000
5.528606	348.788823	5.773005
5.383691	350.776559	5.778010
5.432963	349.354522	5.783014
5.541665	331.708075	5.788019
4.960341	327.970519	5.793024
5.433706	340.068244	5.798029
5.375186	344.418397	5.803034
5.763434	345.189081	5.808038
5.195648	325.732203	5.813043
5.149546	336.193194	5.818048
5.848064	339.508860	5.823053
5.251171	333.154433	5.828058
5.504109	343.680367	5.833062
5.706133	338.992964	5.838067
5.247439	333.205690	5.843072
5.228850	331.700565	5.848077
5.794100	342.637932	5.853082
5.520360	342.636334	5.858086
5.726038	337.844528	5.863091
5.280242	325.937289	5.868096
5.446106	334.811719	5.873101
5.539347	342.829899	5.878106
5.425528	350.431257	5.883110
5.590107	351.346724	5.888115
5.308526	345.969784	5.893120
5.728312	340.821061	5.898125
5.392208	342.953923	5.903130
5.556647	351.429979	5.908134
5.347270	345.948335	5.913139
5.503109	352.754767	5.918144
5.364172	352.716245	5.923149
5.464943	350.601316	5.928154
5.175265	356.534502	5.933158
5.715787	352.846995	5.938163
5.351147	371.691730	5.943168
5.658375	370.586722	5.948173
5.914827	378.985199	5.953178
5.790906	373.770797	5.958182
6.135338	377.975893	5.963187
6.020117	372.361233	5.968192
5.764570	355.661315	5.973197
5.819582	343.305075	5.978202
5.543263	354.560986	5.983206
6.054225	364.344846	5.988211
5.792807	362.290876	5.993216
5.812576	352.521436	5.998221
5.595630	356.909469	6.003226
5.664449	374.126627	6.008230
6.476356	371.185500	6.013235
5.843509	358.262927	6.018240
5.790314	345.276154	6.023245
5.956723	346.294327	6.028250
5.748964	347.628233	6.033254
5.901503	346.651654	6.038259
5.679813	349.917624	6.043264
5.918414	339.664593	6.048269
5.936449	336.677127	6.053274
5.955534	339.767655	6.058278
6.046285	338.455376	6.063283
5.594059	346.196439	6.068288
6.115589	344.122544	6.073293
5.910861	343.737736	6.078298
5.590753	348.478716	6.083302
6.019952	338.656683	6.088307
6.011041	340.702608	6.093312
5.895879	341.071201	6.098317
5.738286	345.650686	6.103322
5.666664	352.912348	6.108326
5.781838	340.162328	6.113331
5.288386	344.215481	6.118336
5.735464	342.455248	6.123341
5.921837	349.337926	6.128346
5.629172	348.929790	6.133350
5.713223	340.831023	6.138355
5.652194	348.022848	6.143360
5.748411	358.561127	6.148365
5.952245	375.737973	6.153370
5.991382	369.220195	6.158374
5.780627	360.071461	6.163379
5.364472	354.705751	6.168384
5.979730	361.138925	6.173389
5.902899	373.097291	6.178394
6.118719	365.403533	6.183398
6.058389	357.154811	6.188403
5.761994	358.563977	6.193408
6.019900	351.016982	6.198413
5.678564	352.768668	6.203418
5.586726	348.157944	6.208422
5.633440	342.302370	6.213427
5.602060	347.394949	6.218432
6.069560	362.628951	6.223437
5.900136	375.546910	6.228442
5.694762	370.708505	6.233446
6.207285	362.149234	6.238451
5.876453	356.931211	6.243456
5.846763	341.566586	6.248461
5.970601	341.253864	6.253466
5.806365	342.475777	6.258470
6.210412	343.279168	6.263475
5.728552	343.829449	6.268480
5.896104	346.951438	6.273485
5.711546	348.603161	6.278490
5.492727	343.046120	6.283494
5.909604	336.552635	6.288499
5.647255	344.538922	6.293504
5.927758	345.577867	6.298509
6.022071	338.230045	6.303514
5.804374	346.311159	6.308518
6.010542	342.375515	6.313523
5.993128	346.440025	6.318528
6.087040	339.699080	6.323533
5.803306	342.696682	6.328538
5.672409	349.968750	6.333542
5.889775	346.962680	6.338547
5.848125	344.924813	6.343552
5.829877	346.738440	6.348557
5.700794	353.179619	6.353562
5.721291	351.894562	6.358566
5.704086	350.848211	6.363571
5.655482	355.511872	6.368576
5.858359	337.707544	6.373581
5.688580	345.090439	6.378586
5.471551	349.283712	6.383590
5.772689	350.375679	6.388595
5.343244	351.724586	6.393600
5.904353	358.389321	6.398605
6.216580	375.916844	6.403610
5.903574	365.102936	6.408614
6.104712	358.561890	6.413619
5.553452	354.969720	6.418624
5.648836	341.203929	6.423629
5.910808	352.424182	6.428634
5.795799	349.365008	6.433638
5.934899	347.021137	6.438643
5.607707	350.671228	6.443648
6.038619	361.262426	6.448653
5.979061	356.317591	6.453658
5.873348	351.956624	6.458662
6.122645	337.003628	6.463667
5.894903	349.118983	6.468672
5.619983	346.750328	6.473677
5.694959	343.454663	6.478682
5.528588	349.508525	6.483686
5.518420	350.584156	6.488691
6.071446	357.672924	6.493696
6.186097	355.941095	6.498701
5.995825	348.673939	6.503706
5.445647	346.318499	6.508710
6.005111	344.291210	6.513715
5.587624	351.488188	6.518720
5.704124	346.954659	6.523725
5.801870	355.496620	6.528730
6.035244	353.801373	6.533734
5.804834	338.641868	6.538739
5.734553	343.233535	6.543744
5.629812	347.307769	6.548749
5.964469	358.012387	6.553754
5.546388	356.204193	6.558758
6.173290	359.055745	6.563763
5.965443	357.964592	6.568768
5.812258	346.277657	6.573773
5.815134	344.845543	6.578778
5.647537	349.881152	6.583782
5.750130	341.492387	6.588787
5.731818	345.958823	6.593792
5.777655	363.802768	6.598797
5.807945	369.729943	6.603802
5.710921	364.988055	6.608806
6.010797	369.590070	6.613811
5.818278	373.398233	6.618816
5.960065	356.755461	6.623821
5.756333	346.873255	6.628826
5.683475	356.329312	6.633830
6.065014	358.318084	6.638835
5.989279	349.762888	6.643840
5.832311	349.879103	6.648845
5.773436	340.063887	6.653850
5.585404	348.258886	6.658854
5.822341	350.753893	6.663859
5.766985	377.152195	6.668864
6.158787	366.468251	6.673869
6.026134	354.670559	6.678874
5.565894	346.431230	6.683878
5.892505	343.761489	6.688883
5.410736	353.763006	6.693888
5.626114	356.324732	6.698893
6.107068	364.277736	6.703898
5.939669	372.208255	6.708902
6.085789	354.753318	6.713907
5.899048	347.889723	6.718912
5.792989	349.166729	6.723917
5.925068	345.316565	6.728922
5.591782	342.219929	6.733926
5.999973	340.578420	6.738931
5.782607	338.572413	6.743936
6.077385	338.754724	6.748941
5.712545	339.365746	6.753946
5.836514	338.216295	6.758950
5.971803	340.367006	6.763955
6.138621	347.478674	6.768960
6.212679	340.778313	6.773965
6.052557	339.282611	6.778970
5.706749	343.653892	6.783974
5.756292	349.810532	6.788979
5.897680	343.679585	6.793984
5.874215	354.036790	6.798989
6.011161	339.934959	6.803994
5.787485	342.695679	6.808998
5.993083	341.540802	6.814003
5.895278	349.165951	6.819008
5.601060	347.916234	6.824013
5.869728	336.846975	6.829018
5.823448	345.339370	6.834022
5.477765	337.379055	6.839027
5.721872	348.183910	6.844032
5.966084	343.809403	6.849037
5.773892	348.719040	6.854042
5.505101	346.652282	6.859046
5.956764	336.029290	6.864051
6.195258	340.638303	6.869056
6.004522	342.064703	6.874061
5.633990	345.547919	6.879066
5.829340	347.776105	6.884070
6.138581	350.013850	6.889075
5.778260	353.366121	6.894080
5.841469	357.032674	6.899085
5.966624	346.735671	6.904090
5.677755	348.883800	6.909094
5.691952	344.680781	6.914099
6.001093	345.791748	6.919104
5.782078	344.685080	6.924109
5.692390	345.764406	6.929114
5.621302	346.785003	6.934118
6.037561	341.229364	6.939123
5.693278	347.125807	6.944128
5.772151	344.955303	6.949133
5.546299	340.146150	6.954138
5.724394	349.663461	6.959142
5.749868	341.796397	6.964147
5.567049	341.773232	6.969152
5.703479	345.070873	6.974157
5.424490	342.798205	6.979162
5.312595	349.082613	6.984166
5.949092	354.332784	6.989171
6.063442	372.551188	6.994176
5.936877	352.488011	6.999181
5.913611	343.687918	7.004186
5.702835	359.179470	7.009190
6.126648	339.940423	7.014195
5.825542	348.166973	7.019200
5.753072	342.652793	7.024205
5.568612	342.879925	7.029210
5.663058	347.153639	7.034214
5.588031	353.823460	7.039219
5.680128	368.366789	7.044224
6.077277	361.405518	7.049229
5.873215	368.322268	7.054234
5.431921	371.325443	7.059238
6.089699	367.022755	7.064243
5.746107	377.303333	7.069248
5.876267	374.123834	7.074253
6.013678	375.936357	7.079258
5.863394	369.760751	7.084262
6.006351	362.211078	7.089267
5.619571	348.128867	7.094272
5.662259	350.930338	7.099277
5.872110	356.753773	7.104282
5.981186	369.859455	7.109286
6.005419	359.078511	7.114291
5.839289	353.263505	7.119296
5.681813	343.602355	7.124301
5.974530	344.032073	7.129306
5.427787	346.699471	7.134310
5.881047	357.942518	7.139315
5.809219	372.228632	7.144320
6.059249	374.378700	7.149325
5.882031	361.075991	7.154330
5.477030	363.735510	7.159334
5.724083	362.726901	7.164339
5.953210	363.631680	7.169344
6.148518	368.481697	7.174349
5.733748	355.262729	7.179354
5.599786	355.035320	7.184358
5.729718	368.180567	7.189363
5.973132	372.046195	7.194368
5.527841	377.908462	7.199373
5.948541	375.209716	7.204378
5.486087	382.789884	7.209382
5.647417	378.399886	7.214387
5.519956	386.858188	7.219392
5.572702	380.493063	7.224397
5.960294	379.703117	7.229402
5.455907	379.231370	7.234406
5.959796	370.650436	7.239411
6.048549	384.828076	7.244416
6.007047	379.690011	7.249421
5.895858	374.678337	7.254426
5.921499	379.022260	7.259430
5.980051	379.517788	7.264435
5.898737	378.775886	7.269440
5.749847	380.074590	7.274445
6.036945	378.471876	7.279450
5.699440	372.500927	7.284454
5.755049	370.424850	7.289459
6.206531	374.777588	7.294464
5.983835	370.618721	7.299469
6.086322	380.924894	7.304474
5.619452	364.195430	7.309478
6.032605	363.345603	7.314483
5.786447	349.676813	7.319488
5.443576	354.392161	7.324493
5.771954	366.941544	7.329498
5.316357	379.790858	7.334502
5.834310	373.867108	7.339507
5.878231	380.873636	7.344512
5.963988	377.859949	7.349517
5.910130	375.464749	7.354522
5.771042	382.364826	7.359526
5.718975	378.214013	7.364531
5.966629	386.520807	7.369536
6.102014	376.063629	7.374541
5.891841	373.703784	7.379546
5.971619	377.193153	7.384550
6.105401	378.751317	7.389555
5.556922	367.110089	7.394560
5.816127	375.490939	7.399565
5.959692	369.258783	7.404570
5.732150	370.205041	7.409574
5.813473	365.601949	7.414579
5.816405	376.548980	7.419584
5.790345	357.281592	7.424589
5.727220	370.204440	7.429594
5.907579	375.973566	7.434598
6.201444	371.467296	7.439603
5.701273	359.494836	7.444608
5.327634	361.615169	7.449613
5.689653	374.005262	7.454618
5.635607	379.244477	7.459622
5.837361	375.925445	7.464627
5.804115	384.802484	7.469632
5.850779	380.621903	7.474637
6.150721	381.608890	7.479642
5.808456	383.488804	7.484646
5.933190	375.427486	7.489651
5.974581	383.388954	7.494656
5.750583	379.607214	7.499661
5.782494	378.283561	7.504666
5.653817	386.347587	7.509670
6.204009	373.122939	7.514675
5.889764	378.567451	7.519680
5.555939	367.978795	7.524685
5.682312	368.938281	7.529690
5.750044	378.855534	7.534694
5.868441	375.282123	7.539699
5.732542	378.948104	7.544704
5.730064	374.762637	7.549709
5.900851	377.137965	7.554714
5.655450	375.424707	7.559718
5.930573	374.708047	7.564723
5.726752	377.424834	7.569728
6.031603	376.406456	7.574733
6.292454	370.151919	7.579738
5.988875	361.670951	7.584742
6.008245	351.866846	7.589747
5.564922	349.634216	7.594752
5.371645	355.550452	7.599757
5.795790	368.084373	7.604762
5.602416	369.992715	7.609766
5.889996	375.009005	7.614771
5.742619	379.448278	7.619776
5.925523	376.567101	7.624781
6.008332	369.390879	7.629786
6.074724	381.337573	7.634790
5.984939	367.544008	7.639795
5.627010	363.118240	7.644800
5.687380	363.735421	7.649805
5.936694	359.620747	7.654810
5.990604	373.222200	7.659814
5.797230	355.316322	7.664819
6.038150	352.413899	7.669824
5.779253	353.892633	7.674829
5.636740	355.755452	7.679834
5.690666	355.909958	7.684838
5.708470	371.808076	7.689843
5.564353	376.421648	7.694848
5.495031	378.282217	7.699853
5.691594	373.559398	7.704858
5.719931	371.898693	7.709862
5.982223	372.089146	7.714867
5.914939	367.345095	7.719872
6.060173	376.479899	7.724877
5.687905	375.243695	7.729882
5.867888	379.982192	7.734886
5.683320	373.980985	7.739891
5.753174	376.846634	7.744896
5.734232	378.112770	7.749901
6.035348	373.806780	7.754906
5.763501	375.411588	7.759910
6.082137	377.794403	7.764915
5.687501	378.811152	7.769920
5.747674	377.810399	7.774925
5.932934	373.914716	7.779930
5.659637	379.954326	7.784934
5.648996	370.559917	7.789939
5.732329	376.972050	7.794944
5.853308	378.434060	7.799949
5.969542	379.417524	7.804954
5.741885	379.260490	7.809958
5.701472	366.081152	7.814963
5.573616	375.138629	7.819968
5.701327	367.360002	7.824973
5.775764	376.384179	7.829978
5.527771	375.082207	7.834982
5.963890	372.670402	7.839987
5.481821	371.302207	7.844992
5.907671	371.985560	7.849997
5.805209	370.369404	7.855002
5.677334	387.763796	7.860006
5.680930	371.498704	7.865011
5.750109	378.264243	7.870016
5.622617	375.585032	7.875021
5.678191	384.426841	7.880026
5.433846	395.175658	7.885030
6.220051	397.299502	7.890035
6.144627	401.374421	7.895040
5.656405	393.667578	7.900045
5.876175	381.267647	7.905050
5.325367	379.547338	7.910054
6.028331	390.828786	7.915059
6.005727	400.199390	7.920064
5.831711	397.385006	7.925069
6.037347	377.957075	7.930074
5.829439	381.113023	7.935078
5.760482	377.307584	7.940083
5.869105	384.389439	7.945088
5.931755	385.706001	7.950093
5.838744	375.204156	7.955098
5.578222	377.865211	7.960102
6.076854	368.619924	7.965107
5.949513	367.309025	7.970112
5.943209	379.786555	7.975117
6.210131	373.920752	7.980122
6.041475	376.966730	7.985139
6.343771	367.491723	7.990157
6.117011	381.200993	7.995174
6.025702	377.432810	8.000192
6.051436	371.643644	8.005210
5.783086	375.373832	8.010227
6.206591	367.127666	8.015245
5.777217	369.707254	8.020262
5.615601	369.186071	8.025280
6.057075	369.414755	8.030298
5.686634	370.360706	8.035315
5.788520	364.582160	8.040333
6.087414	373.327828	8.045350
5.757858	376.397932	8.050368
6.303784	371.690445	8.055386
5.548576	368.141046	8.060403
5.689059	363.490265	8.065421
6.148377	368.240019	8.070438
5.816155	371.842212	8.075456
6.007953	366.900673	8.080474
5.663108	374.009187	8.085491
5.518067	371.643879	8.090509
5.790357	373.523276	8.095526
5.527257	369.937071	8.100544
5.822863	365.494441	8.105562
5.359979	374.539858	8.110579
5.799957	376.079112	8.115597
5.610178	379.021356	8.120614
5.850732	396.472032	8.125632
6.502421	394.086989	8.130650
6.263665	393.138851	8.135667
5.968553	384.502656	8.140685
5.880432	368.254092	8.145702
5.821794	377.779180	8.150720
5.844637	371.590723	8.155738
5.561850	388.269459	8.160755
5.999073	394.620188	8.165773
6.294357	406.288081	8.170790
6.178049	407.882054	8.175808
6.467397	401.448489	8.180826
5.948261	390.531467	8.185843
6.118880	371.776679	8.190861
5.997537	370.482356	8.195878
5.939017	383.335296	8.200896
5.629993	364.221984	8.205914
5.981738	392.662366	8.210931
6.201802	402.270246	8.215949
6.138239	404.914059	8.220966
6.008191	405.012792	8.225984
6.268236	410.464203	8.231002
5.926996	408.285695	8.236019
6.242987	399.734901	8.241037
6.678614	395.436583	8.246054
5.801061	392.375705	8.251072
6.239314	381.866450	8.256090
5.879643	378.924725	8.261107
5.743768	382.434963	8.266125
6.166637	394.598016	8.271142
6.271418	403.558506	8.276160
6.255043	398.776418	8.281178
5.909355	393.773489	8.286195
6.343520	397.108835	8.291213
6.386312	383.963318	8.296230
5.790987	387.755132	8.301248
6.038214	394.139683	8.306266
6.257819	394.879477	8.311283
6.375297	405.321994	8.316301
6.176049	395.515684	8.321318
5.940051	401.548007	8.326336
6.179788	404.299458	8.331354
6.362729	403.214569	8.336371
6.229151	405.155664	8.341389
6.282738	399.242791	8.346406
6.061950	393.704264	8.351424
6.281165	390.253525	8.356442
6.231324	396.969726	8.361459
5.839552	399.633636	8.366477
6.427792	404.448858	8.371494
6.535096	409.268330	8.376512
6.586895	395.545375	8.381530
6.434512	395.059864	8.386547
6.158904	378.865363	8.391565
5.951356	383.547806	8.396582
5.820058	379.485875	8.401600
6.522302	390.392530	8.406618
6.232372	390.480339	8.411635
6.488327	390.015591	8.416653
6.607525	379.682978	8.421670
6.029975	380.129805	8.426688
6.357718	381.505967	8.431706
6.172417	384.037465	8.436723
6.205794	373.363191	8.441741
6.112408	376.566615	8.446758
6.028762	392.107946	8.451776
6.340876	407.919165	8.456794
6.364356	411.284135	8.461811
5.983038	402.252200	8.466829
6.006236	406.362626	8.471846
6.182316	414.398596	8.476864
6.384104	403.564143	8.481882
6.320335	412.257690	8.486899
6.420842	409.524578	8.491917
6.511907	388.584304	8.496934
6.164467	410.780398	8.501952
6.510365	403.136779	8.506970
6.334097	408.876757	8.511987
6.325146	408.465124	8.517005
6.220072	404.195515	8.522022
6.408055	407.265944	8.527040
6.630229	404.751250	8.532058
6.506587	411.084237	8.537075
6.661412	418.173413	8.542093
7.057666	401.811933	8.547110
6.740149	413.094335	8.552128
6.481830	395.567732	8.557146
6.531280	394.647062	8.562163
6.416398	382.924979	8.567181
6.545454	385.070004	8.572199
5.906634	388.779263	8.577216
6.745575	394.027142	8.582234
6.730840	409.709823	8.587251
6.392223	397.817707	8.592269
6.618512	391.300107	8.597287
5.851017	392.340938	8.602304
6.297846	397.526198	8.607322
6.653039	412.775808	8.612339
6.451294	418.865452	8.617357
6.726071	407.096741	8.622375
6.474817	412.334809	8.627392
6.747125	409.407122	8.632410
6.644142	406.113857	8.637427
6.441126	405.522172	8.642445
6.500053	403.632099	8.647463
6.149574	414.813472	8.652480
6.754477	411.277213	8.657498
6.455189	403.228856	8.662515
6.553403	413.532848	8.667533
6.858404	413.666031	8.672551
6.657893	411.511461	8.677568
6.818526	400.238585	8.682586
6.442319	392.386026	8.687603
6.014974	390.933530	8.692621
6.401406	402.839850	8.697639
6.310278	412.183740	8.702656
6.686323	408.909178	8.707674
6.699618	419.737626	8.712691
6.492663	416.189157	8.717709
6.631639	411.590969	8.722727
6.444333	421.942836	8.727744
6.725146	411.229138	8.732762
6.932757	413.249161	8.737779
6.770752	410.127663	8.742797
6.988929	412.713999	8.747815
6.541506	412.036417	8.752832
6.735008	413.757028	8.757850
6.874694	410.314534	8.762867
6.639683	417.400550	8.767885
6.648836	416.014542	8.772903
6.889681	412.306695	8.777920
6.981353	397.141821	8.782938
6.678018	386.617182	8.787955
6.285411	392.457539	8.792973
6.795491	384.050190	8.797991
6.459013	410.356919	8.803008
6.587143	414.860372	8.808026
6.900113	412.800683	8.813043
6.798846	408.500129	8.818061
6.788724	408.268204	8.823079
6.606360	410.812998	8.828096
6.691808	412.090516	8.833114
6.586698	413.931828	8.838131
6.482972	412.719223	8.843149
6.976051	407.758883	8.848167
6.532924	410.452951	8.853184
6.612253	408.888211	8.858202
6.674200	407.202541	8.863219
6.643441	414.970621	8.868237
6.825930	403.414619	8.873255
6.899733	407.672953	8.878272
6.916630	412.724111	8.883290
6.581329	406.645531	8.888307
6.436740	412.838692	8.893325
6.856341	410.510382	8.898343
6.342587	412.155405	8.903360
6.387578	406.197106	8.908378
6.724266	419.521796	8.913395
6.809204	437.827943	8.918413
7.178436	424.158888	8.923431
7.334001	430.764521	8.928448
6.732120	421.853538	8.933466
7.009039	405.245695	8.938483
6.858142	413.664324	8.943501
6.762182	406.423763	8.948519
6.391979	405.730639	8.953536
7.019276	429.468562	8.958554
7.288427	420.168093	8.963571
6.823856	421.244782	8.968589
6.846733	415.323604	8.973607
6.735464	408.007237	8.978624
6.772446	428.529401	8.983642
7.028390	424.575566	8.988659
6.850710	442.973627	8.993677
7.225575	428.737932	8.998695
7.314507	440.037296	9.003712
6.720677	417.334165	9.008730
6.901173	419.635426	9.013747
6.943771	431.648502	9.018765
7.200454	419.244246	9.023783
7.042330	423.311676	9.028800
6.593949	422.491547	9.033818
7.131935	421.849597	9.038835
7.200761	430.460967	9.043853
6.928107	415.526860	9.048871
7.062701	404.818090	9.053888
6.865117	407.153807	9.058906
7.058669	412.942580	9.063923
7.008083	432.900557	9.068941
7.056354	427.392065	9.073959
7.051404	428.249745	9.078976
7.223052	424.832268	9.083994
7.175532	413.687149	9.089011
6.677416	411.718264	9.094029
6.741389	415.251909	9.099047
6.944676	432.747967	9.104064
6.901017	436.791132	9.109082
7.314108	432.534525	9.114099
7.326456	437.784460	9.119117
7.300812	438.438301	9.124135
6.927862	439.037456	9.129152
6.966659	430.032978	9.134170
7.507964	428.827531	9.139187
6.923427	436.031663	9.144205
7.167365	441.662903	9.149223
7.376388	431.344317	9.154240
7.243723	433.494893	9.159258
7.309665	425.120321	9.164275
7.051739	429.946738	9.169293
7.295844	429.906751	9.174311
6.973894	428.461405	9.179328
7.058030	430.452076	9.184346
7.411304	428.848862	9.189363
7.287914	434.160049	9.194381
7.073470	421.875336	9.199399
7.093992	426.215523	9.204416
7.144313	436.089701	9.209434
7.143367	436.300117	9.214451
7.010525	432.981085	9.219469
7.048663	427.843532	9.224487
7.518636	432.712989	9.229504
7.435660	435.124608	9.234522
7.631891	417.412092	9.239539
7.384323	431.088634	9.244557
6.839417	416.178743	9.249575
7.289011	424.191671	9.254592
7.182296	434.520556	9.259610
7.351309	433.820420	9.264627
7.091456	438.061970	9.269645
7.332044	432.512577	9.274663
7.490867	438.326203	9.279680
7.117557	443.296523	9.284698
7.310154	433.001913	9.289715
6.962599	437.837466	9.294733
7.520885	432.578155	9.299751
7.155539	423.886251	9.304768
7.044798	433.303868	9.309786
7.246850	424.619970	9.314803
6.953866	437.301756	9.319821
7.214379	430.571403	9.324839
7.224395	432.978449	9.329856
6.960162	438.755246	9.334874
7.188180	432.169041	9.339891
7.037201	454.738342	9.344909
7.630124	460.113786	9.349927
7.547536	463.850831	9.354944
7.519544	464.875111	9.359962
7.815548	450.273351	9.364979
7.323977	437.110571	9.369997
7.281352	440.224114	9.375015
7.537063	435.987660	9.380032
7.345530	437.121886	9.385050
7.396472	429.161574	9.390067
7.201487	431.063829	9.395085
7.588210	448.589761	9.400103
7.657690	440.910602	9.405120
7.297304	440.322732	9.410138
7.647036	440.261909	9.415155
7.264144	445.723541	9.420173
7.484943	446.568643	9.425191
7.702855	442.227236	9.430208
7.536989	448.142460	9.435226
7.613872	432.115109	9.440243
7.669979	434.179510	9.445261
7.462346	436.757625	9.450279
7.720074	432.970999	9.455296
7.322033	435.884555	9.460314
7.679765	435.816109	9.465331
7.168629	438.590334	9.470349
7.441594	446.781721	9.475367
7.646147	452.480112	9.480384
7.794957	458.802647	9.485402
7.673610	450.180946	9.490419
7.404270	445.843257	9.495437
7.354990	451.390977	9.500455
7.768286	459.574487	9.505472
7.700004	465.223580	9.510490
7.755177	456.908052	9.515507
7.270438	450.926635	9.520525
7.646702	455.928930	9.525543
7.908384	460.816943	9.530560
7.503803	462.162616	9.535578
7.626715	461.185096	9.540595
7.697245	466.577363	9.545613
7.809563	471.451532	9.550631
7.976688	446.838438	9.555648
7.724165	442.201533	9.560666
7.340379	444.874167	9.565683
7.475056	442.646374	9.570701
7.686912	461.186434	9.575719
7.804900	458.426209	9.580736
7.517225	480.593806	9.585754
7.866647	466.977399	9.590771
7.681091	464.475096	9.595789
7.559765	466.021091	9.600807
7.779441	458.369214	9.605824
7.607066	466.816426	9.610842
7.837123	459.373246	9.615859
8.263195	471.472449	9.620877
8.167356	458.308686	9.625895
7.732119	441.392383	9.630912
7.470536	437.415981	9.635930
7.808640	434.891534	9.640947
7.910415	445.220546	9.645965
7.636063	440.507341	9.650983
7.893780	442.795623	9.656000
7.654348	454.026545	9.661018
7.956980	459.026862	9.666035
8.130130	448.236092	9.671053
7.586904	446.397103	9.676071
7.744210	443.990578	9.681088
7.969953	458.385556	9.686106
8.172763	447.599324	9.691123
7.917216	435.750702	9.696141
7.774542	437.448052	9.701159
7.920461	430.937051	9.706176
7.770915	438.901766	9.711194
7.585136	430.362196	9.716211
7.899519	442.422394	9.721229
8.063120	457.255383	9.726247
8.095102	441.999963	9.731264
7.833367	450.365711	9.736282
7.826204	433.856842	9.741299
8.123383	442.338681	9.746317
7.621427	450.328688	9.751335
8.297688	449.611286	9.756352
7.794103	442.217554	9.761370
8.069775	436.746201	9.766387
8.175997	433.963520	9.771405
8.272286	423.916538	9.776423
8.130017	429.142471	9.781440
7.835266	438.761020	9.786458
7.941479	433.440356	9.791475
7.865400	433.370126	9.796493
7.571290	430.543706	9.801511
8.057707	438.230884	9.806528
8.140889	454.737487	9.811546
8.030034	458.268204	9.816563
7.850056	447.314272	9.821581
7.865065	456.182383	9.826599
8.364724	447.634414	9.831616
7.857632	461.172868	9.836634
7.996312	460.212223	9.841651
8.220241	464.287065	9.846669
7.937433	466.009787	9.851687
8.365750	461.319583	9.856704
8.062380	464.233411	9.861722
8.179371	457.564210	9.866739
8.033546	459.252832	9.871757
8.183726	466.688442	9.876775
8.202411	453.093547	9.881792
7.942901	464.781112	9.886810
7.899354	460.685537	9.891827
8.311359	457.757738	9.896845
8.263261	466.932147	9.901863
8.075898	459.516357	9.906880
8.158408	466.840150	9.911898
8.214641	460.425477	9.916915
8.135608	460.688191	9.921933
7.882231	469.777509	9.926951
8.110412	473.146192	9.931968
7.897361	467.038487	9.936986
7.864096	463.620683	9.942003
7.818612	461.821901	9.947021
7.884642	467.975484	9.952039
8.053158	464.843534	9.957056
8.406105	472.025902	9.962074
8.577046	477.013585	9.967091
8.219048	463.242491	9.972109
8.156695	471.063464	9.977127
8.492076	452.585012	9.982144
7.975000	458.299755	9.987162
7.964421	459.398704	9.992179
8.298502	465.202413	9.997197
8.077962	483.191510	10.002215
8.369377	485.106333	10.007232
8.702262	482.522511	10.012250
8.687338	485.423224	10.017267
8.454521	465.591709	10.022285
8.328204	471.191953	10.027303
8.613023	453.776317	10.032320
8.717477	458.452784	10.037338
8.391906	457.070628	10.042355
8.508758	459.857200	10.047373
8.053840	455.547285	10.052391
8.753613	457.779693	10.057408
8.600249	461.964052	10.062426
8.122916	456.232567	10.067443
8.154903	453.721407	10.072461
8.067463	456.839224	10.077479
8.403974	455.774174	10.082496
8.174729	460.494875	10.087514
8.244160	459.903150	10.092531
8.533491	471.670102	10.097549
8.456820	484.928659	10.102567
8.554816	481.539112	10.107584
8.519093	487.583971	10.112602
8.514024	483.521385	10.117619
8.652740	464.019266	10.122637
8.445752	462.429299	10.127655
8.540154	459.067909	10.132672
8.438236	463.402202	10.137690
8.357421	461.900389	10.142707
8.454101	468.474848	10.147725
8.549044	482.461620	10.152743
8.552794	487.988172	10.157760
8.796769	483.048979	10.162778
8.339384	475.462753	10.167795
8.409423	465.342537	10.172813
8.460730	487.429607	10.177831
8.718000	481.790629	10.182848
8.859347	484.440286	10.187866
8.780461	477.147656	10.192883
8.385007	474.861590	10.197901
8.553714	474.308735	10.202919
8.739827	467.465499	10.207936
8.407035	478.936290	10.212954
8.231971	486.038393	10.217971
8.382758	475.659150	10.222989
8.547703	491.962898	10.228007
8.476758	478.376524	10.233024
8.805321	485.847560	10.238042
8.704291	484.374681	10.243059
8.797512	482.482462	10.248077
8.407777	495.120282	10.253095
8.940487	482.716919	10.258112
8.741055	490.080126	10.263130
8.541654	489.109719	10.268147
8.868738	484.477605	10.273165
8.697736	486.060566	10.278183
8.690634	492.091042	10.283200
8.649871	486.007947	10.288218
8.865436	486.819078	10.293235
8.808381	478.642979	10.298253
8.714622	479.860223	10.303271
8.917534	482.627431	10.308288
8.569606	490.574436	10.313306
8.671452	481.671684	10.318323
8.997744	485.252059	10.323341
8.711712	487.714434	10.328359
8.490875	478.420268	10.333376
8.843674	485.191282	10.338394
8.904749	486.742113	10.343411
8.698485	485.648835	10.348429
8.799274	485.996922	10.353447
8.879953	481.750663	10.358464
8.860883	478.820427	10.363482
8.864641	486.247026	10.368499
9.146012	475.330846	10.373517
8.815236	489.484567	10.378535
8.851679	474.164798	10.383552
8.912228	482.568333	10.388570
8.914807	488.275576	10.393587
8.905174	477.102289	10.398605
8.955574	492.594361	10.403623
8.917658	479.328476	10.408640
8.784368	486.251629	10.413658
8.749618	476.475898	10.418675
8.788196	488.523538	10.423693
8.871461	509.366269	10.428711
9.107589	522.054205	10.433728
9.261830	507.718760	10.438746
8.915885	497.996513	10.443763
9.408436	484.602238	10.448781
9.246492	488.399275	10.453799
8.800439	485.953685	10.458816
8.672669	484.513185	10.463834
8.874923	484.134092	10.468851
9.402636	494.285726	10.473869
8.699581	493.937651	10.478887
9.154681	509.872532	10.483904
9.261592	505.727623	10.488922
9.141320	494.199444	10.493939
9.133945	491.718810	10.498957
8.676873	494.493737	10.503975
8.852647	511.285636	10.508992
9.459305	516.898177	10.514010
9.287577	520.856477	10.519027
9.359892	507.606761	10.524045
9.424968	494.169490	10.529063
9.064764	488.518787	10.534080
9.211639	480.881119	10.539098
8.968444	489.523127	10.544115
9.244978	486.574058	10.549133
8.974770	487.054241	10.554151
9.312485	490.861646	10.559168
9.486525	482.867734	10.564186
8.555186	493.380641	10.569203
9.278454	497.313561	10.574221
9.190976	515.471199	10.579239
9.287863	513.444324	10.584256
9.323742	512.366851	10.589274
9.252255	519.365407	10.594291
9.302040	515.387620	10.599309
9.346418	517.373076	10.604327
9.585838	519.973825	10.609344
9.374755	497.492019	10.614362
8.864560	493.415048	10.619379
9.413353	494.898505	10.624397
9.377912	495.413627	10.629415
8.938896	502.709039	10.634432
9.243461	507.015600	10.639450
9.046472	512.907659	10.644467
9.323061	511.468304	10.649485
9.487491	512.935099	10.654503
9.049018	518.449067	10.659520
9.471188	512.875877	10.664538
9.340386	517.621236	10.669555
9.573492	511.619151	10.674573
9.616743	512.122817	10.679591
9.698287	513.899181	10.684608
9.627523	504.500234	10.689626
9.666194	511.305560	10.694643
9.501631	498.668654	10.699661
9.315463	491.990389	10.704679
8.976317	484.080075	10.709696
9.282421	500.400023	10.714714
9.429759	509.593076	10.719731
9.457539	507.718186	10.724749
9.310378	515.573499	10.729767
9.524733	515.668350	10.734784
9.763058	513.234226	10.739802
9.336223	512.270770	10.744819
9.714657	501.880781	10.749837
9.443161	508.774076	10.754855
9.131804	511.355009	10.759872
9.746266	505.463585	10.764890
9.666869	514.245006	10.769907
9.454765	503.193016	10.774925
9.462677	505.282926	10.779943
9.294532	501.899257	10.784960
9.328265	506.305384	10.789978
9.322639	508.824866	10.794995
9.886683	506.009668	10.800013
9.671382	512.231505	10.805031
9.446014	511.395308	10.810048
9.695681	504.526571	10.815066
9.370236	518.251909	10.820083
9.536056	506.773585	10.825101
9.438666	503.608891	10.830119
9.525520	512.958998	10.835136
9.467200	505.105511	10.840154
9.622410	525.961153	10.845171
9.993220	521.065705	10.850189
9.528737	513.071610	10.855207
9.363793	519.501238	10.860224
10.040977	519.946978	10.865242
9.545622	535.139728	10.870259
9.883938	528.793663	10.875277
10.276618	537.622117	10.880295
9.335976	520.466407	10.885312
9.438157	523.169600	10.890330
9.495609	534.352601	10.895347
9.854287	527.437460	10.900365
9.470488	534.266494	10.905383
10.078935	546.097385	10.910400
10.256958	536.214343	10.915418
10.108833	546.485597	10.920435
9.910806	540.560008	10.925453
9.448561	518.657122	10.930471
9.851274	532.364057	10.935488
10.006119	529.864625	10.940506
9.524721	539.212393	10.945523
9.977481	533.831949	10.950541
10.074095	532.219260	10.955559
9.747359	543.754839	10.960576
9.875949	535.133827	10.965594
10.103245	540.166722	10.970611
9.774455	538.239462	10.975629
9.983742	538.362316	10.980647
9.629745	540.201157	10.985664
9.997559	528.369118	10.990682
10.112018	537.651878	10.995699
9.991166	528.914114	11.000717
9.886702	534.236964	11.005735
9.995170	538.570297	11.010752
10.221113	531.947782	11.015770
10.137166	536.784988	11.020787
9.996653	537.436005	11.025805
10.190215	539.071391	11.030823
9.963940	540.244642	11.035840
9.894352	532.570553	11.040858
10.050385	535.603192	11.045875
10.233245	532.734975	11.050893
10.011059	537.594677	11.055911
9.638557	536.548803	11.060928
10.236101	528.561902	11.065946
10.185473	534.875566	11.070963
10.017730	534.705759	11.075981
10.267171	535.831929	11.080999
10.150609	540.995576	11.086016
10.342967	529.474064	11.091034
9.888423	533.195556	11.096051
9.668219	538.879279	11.101069
9.942581	529.022018	11.106087
9.931497	535.029354	11.111104
10.480380	532.236542	11.116122
9.895062	539.652056	11.121139
10.086938	541.931178	11.126157
10.176955	535.969114	11.131175
9.850113	536.508672	11.136192
10.341490	539.879455	11.141210
10.250195	540.230021	11.146227
10.019570	547.992879	11.151245
10.234580	538.809170	11.156263
10.053795	547.881001	11.161280
9.959523	540.629469	11.166298
9.980120	549.320343	11.171315
10.358743	573.390392	11.176333
10.687654	573.645790	11.181351
10.327531	563.087918	11.186368
10.554460	544.132074	11.191386
10.161455	544.824704	11.196403
10.037518	541.398670	11.201421
10.465228	546.242093	11.206439
10.444704	559.539445	11.211456
10.333156	543.398703	11.216474
10.226087	550.116965	11.221491
10.289696	561.535170	11.226509
10.458247	566.321324	11.231527
10.801030	568.829577	11.236544
10.674936	550.501236	11.241562
10.486001	541.319260	11.246579
10.189728	540.169825	11.251597
10.372777	541.157788	11.256615
10.175053	542.105855	11.261632
10.394707	564.138192	11.266650
10.480898	558.235213	11.271667
10.591265	578.181685	11.276685
10.386161	567.677466	11.281703
10.560560	571.254275	11.286720
10.612227	571.439841	11.291738
10.382001	569.991889	11.296755
10.530240	566.345203	11.301773
10.922461	560.570473	11.306791
10.083150	565.199719	11.311808
10.410792	556.539436	11.316826
10.669371	559.440934	11.321843
10.580119	573.910028	11.326861
10.974692	559.151893	11.331879
10.686059	569.693852	11.336896
10.523817	564.696709	11.341914
10.791459	566.297196	11.346931
10.626991	566.266600	11.351949
10.528560	569.459089	11.356967
10.281196	564.013673	11.361984
10.546510	564.041626	11.367002
10.726752	565.460142	11.372019
10.336220	571.648819	11.377037
10.656243	563.375593	11.382055
10.391002	568.122364	11.387072
10.449884	563.431890	11.392090
10.523355	563.733718	11.397107
10.741978	569.795544	11.402125
10.746443	561.168695	11.407143
10.460335	571.391953	11.412160
10.562537	565.456992	11.417178
10.616058	566.021751	11.422195
10.567768	559.547381	11.427213
11.115401	576.185263	11.432231
10.594524	572.026975	11.437248
10.908143	571.226516	11.442266
11.169732	565.424600	11.447283
10.527258	569.544516	11.452301
11.017514	563.777566	11.457319
10.675438	563.807873	11.462336
10.677567	569.878384	11.467354
11.311108	574.935355	11.472371
10.852727	576.179323	11.477389
10.925939	560.933493	11.482407
10.669188	572.897827	11.487424
10.687615	562.562292	11.492442
10.870305	576.528321	11.497459
11.235277	593.234457	11.502477
11.184592	577.956964	11.507495
10.819577	571.939139	11.512512
10.717673	566.687534	11.517530
11.141128	567.779972	11.522547
10.867628	581.850872	11.527565
10.997020	577.752612	11.532583
11.344486	588.149494	11.537600
10.872635	574.419789	11.542618
11.078552	565.944212	11.547635
11.103992	569.209293	11.552653
10.729698	561.631704	11.557671
10.635118	576.204234	11.562688
10.924666	585.736161	11.567706
11.112136	585.447106	11.572723
11.043283	587.496790	11.577741
11.237836	585.720250	11.582759
10.859798	579.033958	11.587776
11.150505	580.115505	11.592794
11.439346	584.344580	11.597811
11.136130	581.916658	11.602829
11.283631	585.446156	11.607847
11.489509	588.826235	11.612864
11.417138	584.411013	11.617882
11.141835	570.291114	11.622899
10.837590	569.422898	11.627917
11.269689	571.445530	11.632935
10.910557	582.334581	11.637952
11.529741	589.699872	11.642970
11.363224	582.889583	11.647987
10.938159	591.033453	11.653005
11.422779	581.376563	11.658023
11.256123	584.022124	11.663040
11.182672	584.111486	11.668058
10.768139	582.992259	11.673075
11.035716	592.981930	11.678093
11.413961	583.200931	11.683111
11.303276	582.009149	11.688128
11.396266	584.932756	11.693146
11.614032	582.731143	11.698163
11.338270	584.290124	11.703181
11.293902	582.393316	11.708199
11.370190	584.482937	11.713216
11.452396	577.287593	11.718234
11.774388	580.698833	11.723251
10.981549	585.676466	11.728269
11.374834	576.059307	11.733287
11.370671	581.780693	11.738304
11.143502	584.306165	11.743322
11.643528	585.735506	11.748339
11.414102	585.623153	11.753357
11.532555	587.261927	11.758375
11.261645	585.931529	11.763392
11.192013	582.148487	11.768410
11.409521	575.237804	11.773427
11.486479	577.906800	11.778445
11.617440	571.750947	11.783463
11.721457	576.774743	11.788480
11.251027	583.840765	11.793498
11.618902	574.791357	11.798515
11.246719	592.702548	11.803533
11.758620	583.471424	11.808551
12.038819	579.120255	11.813568
11.496946	581.905696	11.818586
11.723184	584.720632	11.823603
11.587049	583.198836	11.828621
11.593896	580.845744	11.833639
11.573615	583.892431	11.838656
11.646924	581.889922	11.843674
11.420273	580.761237	11.848691
11.165607	587.333496	11.853709
11.570572	580.103405	11.858727
11.293275	584.625422	11.863744
11.616856	608.897738	11.868762
12.049544	602.698210	11.873779
11.830390	593.079506	11.878797
11.603923	588.801208	11.883815
11.803716	579.725500	11.888832
11.605262	581.139012	11.893850
11.487079	590.032010	11.898867
11.686319	609.843933	11.903885
11.881386	607.290785	11.908903
11.744224	610.830617	11.913920
11.813899	610.826993	11.918938
11.929952	607.816292	11.923955
11.879575	610.240452	11.928973
11.864804	609.083766	11.933991
12.126823	611.557963	11.939008
11.888038	607.454916	11.944026
12.401297	596.168584	11.949043
11.791672	593.225294	11.954061
11.804270	578.333948	11.959079
11.688856	579.843938	11.964096
11.658688	585.119860	11.969114
12.047194	589.760158	11.974131
11.842011	601.367772	11.979149
12.267205	599.192829	11.984167
12.116002	586.391840	11.989184
11.932051	585.275177	11.994202
11.939904	571.516629	11.999219
11.686121	575.793428	12.004237
12.201583	594.957935	12.009255
12.396736	596.100382	12.014272
11.849566	584.277298	12.019290
11.739481	575.163146	12.024307
11.915331	603.319876	12.029325
11.950642	605.016707	12.034343
12.051688	599.560828	12.039360
12.246198	605.183187	12.044378
12.552167	596.852039	12.049395
12.071187	604.916796	12.054413
11.919558	607.107344	12.059431
11.933346	603.481732	12.064448
11.770030	611.583845	12.069466
12.045580	611.727222	12.074483
12.133099	609.551897	12.079501
11.936732	607.483023	12.084519
12.293146	610.700985	12.089536
12.253243	600.762261	12.094554
12.274407	595.843393	12.099571
11.893777	598.499585	12.104589
12.149327	607.586990	12.109607
12.280307	598.215402	12.114624
12.071829	604.297180	12.119642
12.249948	598.096503	12.124659
12.162216	602.290307	12.129677
12.243358	602.764870	12.134695
12.235745	595.544037	12.139712
11.861171	612.294901	12.144730
12.202317	598.479173	12.149747
12.032330	603.620980	12.154765
12.240527	613.687225	12.159783
12.285578	628.679960	12.164800
12.505847	634.164216	12.169818
12.626678	632.201663	12.174835
12.661694	627.651726	12.179853
12.467809	615.447307	12.184871
12.332169	608.073468	12.189888
12.318125	608.047489	12.194906
12.364972	616.810821	12.199923
12.579745	625.204642	12.204941
12.851545	619.873424	12.209959
12.410117	607.537177	12.214976
12.308864	612.135556	12.219994
12.451156	605.071185	12.225011
12.302311	610.373852	12.230029
12.569507	623.175223	12.235047
12.904428	620.387906	12.240064
12.428546	610.845163	12.245082
12.765774	597.230464	12.250099
12.381224	596.899720	12.255117
12.431380	613.400741	12.260135
12.909231	620.381604	12.265152
12.495676	616.817302	12.270170
12.483198	605.810326	12.275187
12.728866	632.104496	12.280205
12.892782	623.196109	12.285223
12.641321	600.364957	12.290240
12.498212	603.032998	12.295258
12.684150	605.387321	12.300275
12.406679	617.500583	12.305293
12.628823	627.795614	12.310311
12.994284	626.870434	12.315328
12.888442	627.902696	12.320346
12.995550	620.592978	12.325363
12.531637	614.273425	12.330381
12.557626	617.981899	12.335399
12.889590	626.370095	12.340416
12.638413	634.665891	12.345434
13.060663	626.752450	12.350451
12.672132	628.626545	12.355469
12.703998	623.112236	12.360487
12.944870	627.982293	12.365504
13.040299	635.181397	12.370522
12.971402	619.444705	12.375539
12.953709	620.483037	12.380557
12.667967	615.482707	12.385575
12.854502	616.613985	12.390592
12.950279	622.966234	12.395610
12.904525	618.704852	12.400627
12.937094	624.557366	12.405645
13.028225	620.097739	12.410663
13.250422	627.125859	12.415680
12.729529	618.837920	12.420698
13.048156	615.237019	12.425715
13.222514	630.355972	12.430733
12.787589	613.267196	12.435751
12.886663	613.667535	12.440768
13.073432	622.095124	12.445786
13.182233	629.433734	12.450803
12.571020	623.792459	12.455821
12.590015	625.346335	12.460839
13.101410	624.538320	12.465856
12.766656	636.419563	12.470874
12.909913	632.355408	12.475891
12.932238	630.458376	12.480909
12.863805	625.176013	12.485927
12.743785	621.869186	12.490944
12.987544	630.654444	12.495962
12.855942	635.332653	12.500979
13.062924	638.635991	12.505997
13.169654	659.632312	12.511015
13.552419	647.154049	12.516032
13.458696	660.744101	12.521050
13.518605	639.836991	12.526067
13.845033	628.244390	12.531085
13.030783	630.264563	12.536103
13.312675	620.800458	12.541120
13.261149	631.340990	12.546138
12.962623	626.584096	12.551155
13.110718	626.985176	12.556173
12.927803	624.934543	12.561191
13.327405	629.342914	12.566208
13.299867	641.791163	12.571226
13.672549	642.359568	12.576243
13.360407	634.323454	12.581261
12.783684	634.440249	12.586279
13.337077	642.042626	12.591296
13.554301	648.635388	12.596314
13.684069	652.258974	12.601331
13.926831	652.036939	12.606349
13.477677	638.334322	12.611367
13.412209	621.545555	12.616384
13.196933	627.724130	12.621402
13.205958	635.778430	12.626419
13.337186	638.145950	12.631437
13.326917	652.162501	12.636455
13.883087	652.372200	12.641472
13.812083	649.072604	12.646490
13.548915	645.888484	12.651507
13.382543	644.592933	12.656525
13.648867	649.792225	12.661543
13.922431	650.716194	12.666560
13.741857	639.380360	12.671578
13.457003	624.426813	12.676595
13.667783	622.932405	12.681613
13.274165	637.293700	12.686631
13.377449	645.660524	12.691648
13.849410	648.180273	12.696666
13.857001	648.525096	12.701683
13.811997	643.447102	12.706701
13.542027	649.612696	12.711719
13.817189	647.796426	12.716736
13.666875	660.742547	12.721754
13.745066	645.606234	12.726771
14.068392	649.871740	12.731789
13.417261	647.327216	12.736807
13.642146	647.094953	12.741824
13.783864	647.914581	12.746842
13.950684	646.083773	12.751859
13.921036	643.239897	12.756877
13.809899	649.743734	12.761895
14.194540	643.988535	12.766912
13.679775	647.452327	12.771930
13.764978	651.018335	12.776947
14.123874	644.743221	12.781965
13.731588	647.521029	12.786983
14.057433	643.187676	12.792000
13.914592	644.491598	12.797018
13.840118	648.042513	12.802035
13.936943	644.838939	12.807053
13.913320	635.097877	12.812071
13.965454	636.170708	12.817088
13.998923	642.573437	12.822106
14.130505	639.305057	12.827123
14.234358	640.115798	12.832141
13.903056	635.925707	12.837159
13.979769	626.853029	12.842176
13.964317	635.653457	12.847194
13.706166	643.355965	12.852211
14.241229	637.933316	12.857229
14.153003	646.381849	12.862247
14.421601	641.124377	12.867264
14.368792	638.626834	12.872282
14.236051	631.958952	12.877299
14.224882	618.012187	12.882317
13.710023	616.516093	12.887335
14.226509	620.750787	12.892352
14.090847	636.997779	12.897370
14.156905	640.245520	12.902387
14.184220	635.887591	12.907405
14.097995	642.899076	12.912423
14.058724	641.565945	12.917440
14.569105	642.619390	12.922458
14.120598	641.322135	12.927475
14.616707	634.353681	12.932493
14.358253	644.427929	12.937511
14.423847	639.452284	12.942528
14.329225	636.233368	12.947546
14.308342	635.729617	12.952563
14.189526	623.902301	12.957581
14.248387	653.036499	12.962599
14.385020	644.027900	12.967616
14.349221	639.347175	12.972634
14.362188	650.991533	12.977651
14.429819	632.729631	12.982669
14.505509	635.089419	12.987687
14.517302	633.849795	12.992704
14.618706	639.647220	12.997722
14.333517	641.136906	13.002739
14.586862	633.487241	13.007757
14.620381	641.408560	13.012775
14.483126	633.928290	13.017792
14.500778	643.575348	13.022810
14.515979	639.721949	13.027827
14.787674	645.392169	13.032845
14.290343	644.751183	13.037863
14.581441	641.425683	13.042880
14.521413	638.389411	13.047898
14.485836	639.109861	13.052915
14.451005	631.368161	13.057933
14.346409	641.030933	13.062951
14.235898	633.515725	13.067968
14.038550	634.843041	13.072986
13.954202	638.690254	13.078003
14.372248	639.703284	13.083021
14.543185	659.050894	13.088039
14.603278	667.828989	13.093056
14.585876	662.050401	13.098074
14.692006	664.513413	13.103091
14.801435	661.019972	13.108109
14.775315	671.319923	13.113127
14.759539	668.498154	13.118144
14.648311	665.256195	13.123162
14.680497	674.558763	13.128179
15.134857	656.573523	13.133197
14.460671	672.379246	13.138215
14.809995	667.857366	13.143232
14.964749	664.546957	13.148250
14.548445	672.153430	13.153267
14.432996	660.961904	13.158285
14.722927	663.229729	13.163303
14.906622	662.929685	13.168320
14.902848	668.061904	13.173338
14.688992	673.042506	13.178355
15.204531	679.034345	13.183373
15.298332	681.050219	13.188391
15.031620	665.062592	13.193408
14.979723	661.821046	13.198426
15.130755	671.480679	13.203443
15.248899	657.016633	13.208461
15.153759	671.477345	13.213479
15.111084	659.362215	13.218496
15.095944	660.038340	13.223514
14.950138	662.646606	13.228531
15.302262	659.622000	13.233549
15.486972	662.247186	13.238567
15.274327	656.146818	13.243584
15.308257	660.256520	13.248602
15.385180	673.501420	13.253619
15.338862	659.255930	13.258637
15.241695	669.137160	13.263655
15.268481	662.712319	13.268672
15.482050	665.921468	13.273690
14.935275	668.787258	13.278707
15.155124	657.379989	13.283725
14.982794	658.416175	13.288743
15.107993	657.487868	13.293760
15.263245	662.668157	13.298778
15.042020	663.829558	13.303795
15.282229	650.583413	13.308813
15.168156	653.883424	13.313831
15.299106	663.687313	13.318848
15.283267	650.122370	13.323866
15.254706	661.888763	13.328883
15.680502	665.827090	13.333901
15.538282	662.044237	13.338919
15.033525	660.537017	13.343936
15.493846	664.443251	13.348954
15.160586	683.617113	13.353971
14.900370	682.651644	13.358989
15.478374	692.504157	13.364007
15.126480	688.588310	13.369024
15.493125	683.646852	13.374042
15.502471	689.939035	13.379059
15.414640	678.979522	13.384077
15.268673	688.844043	13.389095
15.584732	684.678628	13.394112
15.682656	682.361814	13.399130
15.430314	687.634405	13.404147
15.662472	682.762062	13.409165
15.491653	691.390229	13.414183
15.188578	686.824608	13.419200
16.065120	690.956005	13.424218
15.488600	685.969550	13.429235
15.865020	683.432224	13.434253
15.704063	686.679969	13.439271
15.465401	683.339430	13.444288
15.886352	687.606891	13.449306
15.825585	686.646977	13.454323
15.744192	691.434992	13.459341
15.699349	685.792426	13.464359
15.619888	691.161187	13.469376
16.284037	695.136033	13.474394
15.787664	690.168194	13.479411
15.916773	682.360348	13.484429
15.749274	685.637915	13.489447
16.092038	674.803549	13.494464
15.774008	676.637630	13.499482
15.746138	682.894638	13.504499
15.882682	681.991416	13.509517
15.669357	687.121728	13.514535
16.038485	705.197289	13.519552
16.545124	698.222929	13.524570
15.831384	700.948468	13.529587
15.911134	683.451380	13.534605
15.903202	693.608383	13.539623
15.735911	699.758963	13.544640
16.232739	704.460293	13.549658
16.116904	702.778046	13.554675
16.216757	696.582023	13.559693
16.195333	691.796939	13.564711
15.759859	690.510513	13.569728
16.481658	696.076893	13.574746
15.963223	701.582906	13.579763
16.214028	700.337163	13.584781
16.229390	702.296347	13.589799
16.039349	699.243405	13.594816
16.559187	703.510636	13.599834
16.273539	687.838897	13.604851
16.155276	679.953123	13.609869
16.345233	676.543188	13.614887
16.154125	675.424554	13.619904
16.147859	668.712684	13.624922
16.155311	694.133865	13.629939
16.209041	701.396595	13.634957
16.573959	700.668930	13.639975
16.450411	713.859466	13.644992
16.730282	695.671788	13.650010
16.478238	687.740844	13.655027
16.189159	680.454578	13.660045
16.495344	673.082346	13.665063
16.357888	681.206984	13.670080
16.547619	665.069373	13.675098
16.006188	673.858301	13.680115
16.212210	684.360160	13.685133
16.546251	697.580812	13.690151
16.509799	697.394774	13.695168
16.486295	705.006887	13.700186
16.556104	704.483983	13.705203
16.808164	709.306547	13.710221
16.653449	704.690766	13.715239
16.543647	713.630475	13.720256
16.770211	700.979226	13.725274
16.631850	702.504444	13.730291
16.679297	696.972962	13.735309
16.785685	701.278341	13.740327
16.515332	694.309420	13.745344
16.767050	692.637569	13.750362
16.388148	693.616432	13.755379
16.434730	691.627784	13.760397
16.915817	711.574457	13.765415
16.516538	710.910736	13.770432
17.112198	695.614679	13.775450
16.839946	703.636460	13.780467
16.745053	701.782646	13.785485
16.923664	703.130190	13.790503
16.397630	705.166029	13.795520
16.857972	704.901273	13.800538
16.800747	697.299460	13.805555
16.951075	701.652284	13.810573
16.910377	700.250097	13.815591
16.728860	703.725646	13.820608
17.130298	703.452928	13.825626
16.927404	697.557806	13.830643
16.943393	702.074204	13.835661
16.968229	698.286120	13.840679
17.048228	703.682808	13.845696
16.949160	698.591701	13.850714
17.024533	701.116502	13.855731
16.764547	707.129294	13.860749
17.141953	702.464770	13.865767
17.123313	705.894059	13.870784
17.188512	704.068457	13.875802
17.010605	706.218689	13.880819
16.802649	699.387062	13.885837
17.001471	699.760454	13.890855
17.507691	701.712764	13.895872
17.021703	705.549339	13.900890
17.060310	704.805631	13.905907
17.209151	699.298695	13.910925
17.422580	700.493239	13.915943
17.078671	702.961884	13.920960
16.962925	705.925392	13.925978
17.344928	703.541460	13.930995
17.087375	713.837046	13.936013
17.367000	708.455686	13.941031
17.253420	716.106340	13.946048
16.976714	703.462049	13.951066
17.080460	709.219351	13.956083
16.854230	705.211043	13.961101
17.338424	704.193566	13.966119
17.090372	707.426211	13.971136
17.280466	710.822119	13.976154
17.560161	727.650390	13.981171
17.684668	728.092777	13.986189
17.545551	716.417365	13.991207
17.272421	711.423970	13.996224
17.689132	714.470169	14.001242
17.310845	709.733542	14.006259
17.423260	724.671518	14.011277
17.854142	733.343768	14.016295
17.436498	731.813062	14.021312
17.855405	717.507215	14.026330
17.742139	710.017818	14.031347
17.358721	705.084416	14.036365
17.481411	700.948260	14.041383
17.760697	722.540071	14.046400
17.501048	719.116391	14.051418
17.594618	727.540573	14.056435
17.644453	731.781314	14.061453
17.886654	723.171698	14.066471
17.690548	721.974366	14.071488
17.743318	726.548850	14.076506
18.098880	729.481169	14.081523
17.550029	719.221549	14.086541
17.592798	702.926157	14.091559
17.558826	715.240500	14.096576
17.881968	712.462400	14.101594
17.802734	721.948593	14.106611
17.811633	726.049662	14.111629
17.963186	720.261972	14.116647
17.852921	726.076369	14.121664
17.847998	728.168435	14.126682
18.103482	722.705639	14.131699
17.901553	718.535046	14.136717
17.922303	716.475479	14.141735
17.539120	716.605106	14.146752
17.729065	727.559629	14.151770
17.762118	720.885317	14.156787
17.729344	728.197026	14.161805
17.961539	723.592365	14.166823
17.802744	734.080261	14.171840
17.929314	731.398483	14.176858
17.926873	733.553520	14.181875
17.931475	746.398081	14.186893
18.272458	746.873518	14.191911
18.067087	751.424616	14.196928
18.464250	746.158024	14.201946
18.508654	728.978923	14.206963
17.997251	730.197826	14.211981
18.507268	717.474827	14.216999
18.484692	718.897415	14.222016
18.119910	711.228024	14.227034
18.247601	713.222543	14.232051
18.106641	714.541119	14.237069
18.401287	714.136882	14.242087
18.318361	714.233325	14.247104
17.978348	713.664902	14.252122
18.243724	723.499915	14.257139
18.702314	731.317629	14.262157
18.319631	728.773715	14.267175
18.480067	719.726881	14.272192
18.741576	730.640424	14.277210
18.675916	711.907616	14.282227
18.297688	721.104755	14.287245
18.771610	726.412210	14.292263
18.363569	716.066681	14.297280
18.536225	724.526976	14.302298
18.438954	717.987230	14.307315
18.236265	717.836198	14.312333
18.275334	714.798068	14.317351
18.607710	729.591760	14.322368
18.770433	740.352780	14.327386
18.925829	744.044187	14.332403
18.628521	724.354506	14.337421
19.079421	724.697969	14.342439
18.426111	723.832625	14.347456
18.527811	714.203037	14.352474
18.732395	720.193630	14.357491
18.512593	731.625427	14.362509
18.923604	733.112433	14.367527
18.620239	737.265211	14.372544
18.819801	734.287505	14.377562
18.652271	738.246542	14.382579
18.772162	740.582887	14.387597
19.046171	734.470996	14.392615
18.830093	736.433470	14.397632
18.890694	733.925991	14.402650
18.961409	733.626544	14.407667
18.798921	737.594588	14.412685
19.073130	728.947782	14.417703
18.947307	741.758821	14.422720
18.330681	736.954963	14.427738
18.890030	740.660185	14.432755
18.766337	740.361435	14.437773
19.061620	739.312642	14.442791
18.626239	741.380717	14.447808
18.928615	744.248622	14.452826
19.098354	742.148241	14.457843
19.202799	746.529540	14.462861
19.389022	738.261449	14.467879
19.165525	749.871419	14.472896
18.978054	735.269136	14.477914
19.401436	732.678359	14.482931
18.860179	741.189951	14.487949
19.117576	730.599983	14.492967
19.277444	731.660493	14.497984
19.387245	731.433310	14.503002
19.217151	728.436897	14.508019
18.952002	726.966762	14.513037
19.105091	731.284888	14.518055
19.077457	731.126128	14.523072
19.353295	747.746017	14.528090
19.447710	745.010115	14.533107
19.221045	746.755459	14.538125
19.402383	747.482907	14.543143
19.419191	754.902948	14.548160
19.599900	759.772380	14.553178
19.709055	755.743168	14.558195
19.354881	746.022519	14.563213
19.231933	725.786673	14.568231
19.365496	740.880996	14.573248
19.489716	752.280645	14.578266
19.518543	755.516664	14.583283
19.550668	764.913188	14.588301
19.933385	755.716935	14.593319
19.897262	757.581901	14.598336
19.518377	735.890479	14.603354
19.545906	726.110970	14.608371
19.670327	742.625225	14.613389
19.835898	738.232366	14.618407
19.419706	733.220135	14.623424
19.565638	750.295369	14.628442
19.826544	755.748729	14.633459
19.825233	752.686571	14.638477
20.073642	744.558958	14.643495
20.002760	733.737929	14.648512
19.745438	721.363232	14.653530
20.032294	719.696189	14.658547
19.789473	721.372556	14.663565
19.877065	718.774001	14.668583
19.928275	720.293813	14.673600
19.752820	721.274028	14.678618
19.885878	716.095270	14.683635
19.969760	723.900228	14.688653
19.984839	718.956739	14.693671
19.972680	722.129462	14.698688
19.932427	730.570294	14.703706
20.297229	720.147576	14.708723
19.844191	724.098377	14.713741
19.831551	731.826019	14.718759
20.044377	730.112182	14.723776
19.993912	746.057010	14.728794
20.347568	742.958911	14.733811
20.266294	750.114105	14.738829
20.080548	744.053930	14.743847
19.995157	736.088673	14.748864
19.976465	746.928160	14.753882
20.259722	746.889171	14.758899
19.836098	756.322968	14.763917
20.142038	756.663665	14.768935
20.336983	746.020252	14.773952
20.411787	758.653605	14.778970
20.122173	747.387711	14.783987
20.394680	753.754842	14.789005
20.140630	749.809393	14.794023
20.343469	752.390651	14.799040
20.359940	753.308381	14.804058
20.607676	746.520956	14.809075
20.133462	748.763167	14.814093
20.193161	746.666440	14.819111
20.439870	739.202851	14.824128
20.217305	742.704101	14.829146
20.243373	747.570004	14.834163
20.211535	749.955488	14.839181
20.376231	760.596911	14.844199
20.225294	772.566121	14.849216
20.492361	780.800984	14.854234
20.502903	773.167835	14.859251
20.525846	780.219176	14.864269
20.582575	773.377151	14.869287
20.780137	770.882812	14.874304
20.457763	776.417407	14.879322
20.729724	773.729657	14.884339
20.620248	778.984921	14.889357
20.174030	777.382567	14.894375
20.884304	771.112996	14.899392
20.762921	778.468927	14.904410
20.851225	773.517626	14.909427
20.767718	772.260702	14.914445
20.854264	781.448631	14.919463
20.806484	770.690676	14.924480
21.086074	775.891752	14.929498
21.083545	770.211048	14.934515
21.075108	771.569099	14.939533
20.759983	778.870501	14.944551
21.022873	775.901985	14.949568
20.648110	775.377107	14.954586
21.168608	763.363710	14.959603
20.909407	779.973021	14.964621
20.880297	777.907136	14.969639
21.046446	769.134114	14.974656
20.960691	763.951023	14.979674
21.118789	768.652165	14.984691
20.825872	769.082575	14.989709
21.128921	786.876671	14.994727
21.543318	789.300077	14.999744
20.973661	785.043119	15.004762
21.437126	774.328848	15.009779
21.385959	775.078262	15.014797
21.180622	773.195486	15.019815
21.383193	771.402245	15.024832
21.238208	766.381707	15.029850
21.432646	767.029040	15.034867
21.159594	770.514641	15.039885
21.255947	762.294094	15.044903
21.258547	780.083604	15.049920
21.326798	792.444464	15.054938
21.840195	797.568645	15.059955
21.678901	788.886443	15.064973
21.231002	781.219757	15.069991
21.608789	771.529064	15.075008
21.581966	765.997652	15.080026
21.364891	766.278897	15.085043
21.358430	768.787340	15.090061
21.410891	781.801949	15.095079
21.576165	786.150747	15.100096
21.642787	792.691741	15.105114
22.150052	788.300948	15.110131
21.979691	782.516148	15.115149
21.271353	769.691713	15.120167
21.943219	755.632118	15.125184
21.331264	757.761713	15.130202
21.454658	763.081949	15.135219
21.668947	789.441029	15.140237
21.895055	780.995848	15.145255
22.180194	784.805538	15.150272
21.595257	801.146385	15.155290
21.952918	790.072478	15.160307
22.068770	789.289206	15.165325
21.540113	777.740055	15.170343
21.720903	778.027071	15.175360
21.776242	787.955955	15.180378
21.779918	788.493938	15.185395
21.871208	794.958412	15.190413
21.791009	790.601904	15.195431
22.250779	792.500898	15.200448
21.957852	800.277347	15.205466
22.054196	799.721308	15.210483
22.080681	789.609667	15.215501
21.657714	798.041470	15.220519
22.147266	795.622000	15.225536
21.828005	798.348374	15.230554
21.624335	787.563467	15.235571
22.096261	806.111074	15.240589
22.229832	800.475929	15.245607
21.968533	799.221672	15.250624
21.774815	805.236914	15.255642
22.284773	806.011128	15.260659
22.363421	816.009394	15.265677
22.139481	827.008506	15.270695
22.528330	806.299642	15.275712
22.661745	828.955461	15.280730
22.651847	810.530606	15.285747
22.531557	791.682738	15.290765
22.320765	796.468985	15.295783
22.561680	776.430682	15.300800
22.058567	782.601864	15.305818
22.432654	781.071937	15.310835
22.856966	792.385708	15.315853
22.287009	792.404143	15.320871
22.497122	782.691998	15.325888
22.725035	800.204474	15.330906
22.575368	799.088416	15.335923
22.777226	782.120966	15.340941
22.786574	786.498733	15.345959
22.558663	779.923902	15.350976
22.698421	784.679658	15.355994
22.657489	783.310178	15.361011
22.664285	785.498337	15.366029
22.446205	789.213015	15.371047
22.625163	790.044398	15.376064
22.673224	811.319917	15.381082
22.744366	810.375946	15.386099
23.082377	802.936970	15.391117
22.799284	810.156316	15.396135
23.274865	809.462682	15.401152
22.878729	812.623418	15.406170
22.957674	803.682149	15.411187
23.222680	807.394396	15.416205
22.617651	799.660023	15.421223
23.036288	794.708346	15.426240
23.017325	805.001886	15.431258
23.197448	806.300766	15.436275
23.220527	800.394564	15.441293
22.688945	799.329147	15.446311
23.004866	797.943882	15.451328
23.024888	812.609463	15.456346
22.948681	808.259769	15.461363
23.165929	805.590914	15.466381
22.908782	806.014615	15.471399
22.961807	802.553315	15.476416
22.802051	808.754262	15.481434
22.861485	802.596384	15.486451
22.894617	805.686038	15.491469
22.843040	815.025985	15.496487
23.125090	823.836704	15.501504
23.384688	837.337899	15.506522
23.564173	836.735416	15.511539
23.748951	837.357581	15.516557
23.163496	833.117791	15.521575
23.543651	833.872557	15.526592
23.388804	831.996766	15.531610
23.323270	822.315672	15.536627
23.690883	823.583903	15.541645
23.507704	827.654603	15.546663
23.781756	816.068960	15.551680
23.666709	811.909150	15.556698
23.626146	804.560415	15.561715
23.751034	801.882841	15.566733
23.274446	793.681559	15.571751
23.806995	803.907398	15.576768
23.790048	812.103484	15.581786
23.613413	800.520829	15.586803
24.126246	798.221906	15.591821
23.745609	808.180476	15.596839
23.877178	796.017294	15.601856
23.681791	798.818427	15.606874
23.718182	794.420566	15.611891
23.917606	791.343665	15.616909
23.515974	799.002295	15.621927
23.832354	808.720262	15.626944
23.933823	820.485126	15.631962
23.834286	826.298571	15.636979
24.285052	824.953964	15.641997
24.164584	825.181814	15.647015
24.052026	808.325449	15.652032
23.849395	803.294367	15.657050
23.644150	822.945010	15.662067
24.120826	823.465695	15.667085
24.039752	828.722571	15.672103
24.360219	820.771559	15.677120
24.252028	831.408614	15.682138
23.888918	833.938329	15.687155
24.049225	829.239640	15.692173
23.962597	834.622235	15.697191
24.162737	837.155531	15.702208
24.054312	836.033429	15.707226
23.878884	838.242714	15.712243
24.347659	833.201625	15.717261
23.970056	829.317949	15.722279
24.150912	826.957856	15.727296
24.010462	844.392014	15.732314
23.941290	849.785502	15.737331
24.458586	844.869439	15.742349
24.457591	853.123138	15.747367
24.527325	852.082553	15.752384
24.562500	853.990840	15.757402
24.440581	853.546920	15.762419
24.643544	851.485509	15.767437
24.671842	853.611065	15.772455
24.801746	848.752847	15.777472
24.887386	848.478878	15.782490
25.087911	848.197697	15.787507
25.149328	819.271038	15.792525
24.810517	829.294739	15.797543
24.865091	816.792733	15.802560
25.095910	816.200648	15.807578
24.959321	813.118361	15.812595
24.917176	806.572598	15.817613
24.808389	808.867689	15.822631
24.824420	807.901350	15.827648
24.724448	810.866991	15.832666
24.555106	809.910875	15.837683
24.801685	812.217986	15.842701
24.681909	805.021336	15.847719
24.657079	814.958394	15.852736
24.630446	812.963350	15.857754
24.668426	814.447570	15.862771
24.791942	827.556745	15.867789
24.870518	844.360968	15.872807
25.083019	839.323731	15.877824
25.287632	844.965175	15.882842
25.103617	842.648961	15.887859
25.504278	841.351230	15.892877
25.187692	841.609192	15.897895
24.933035	846.860960	15.902912
25.097809	844.960196	15.907930
24.953601	844.177465	15.912947
25.060132	836.477606	15.917965
25.046029	849.609193	15.922983
25.320242	845.752222	15.928000
25.257266	849.727044	15.933018
25.213732	844.329860	15.938035
25.524328	838.267379	15.943053
25.413154	837.801602	15.948071
25.028017	839.273212	15.953088
25.299441	837.409511	15.958106
25.292822	847.171537	15.963123
25.307212	845.823991	15.968141
25.529022	864.619766	15.973159
25.795946	865.113375	15.978176
25.945658	858.937376	15.983194
25.362606	843.711551	15.988211
25.481241	846.046152	15.993229
25.627547	855.868683	15.998247
25.913277	867.399147	16.003264
26.035887	869.769311	16.008282
25.630192	841.176636	16.013299
25.506702	836.737918	16.018317
25.446053	847.069489	16.023335
25.839152	847.030029	16.028352
25.857854	856.044207	16.033370
25.776106	854.031119	16.038387
26.059735	851.850058	16.043405
25.979192	855.343170	16.048423
26.042774	853.103668	16.053440
26.220447	849.831155	16.058458
26.173976	850.795926	16.063475
26.404811	850.500672	16.068493
25.934428	835.755384	16.073511
26.032985	830.255941	16.078528
26.031751	827.395319	16.083546
25.656564	837.698656	16.088563
26.187586	849.930182	16.093581
26.391687	856.986994	16.098599
25.715879	862.749424	16.103616
26.367898	855.196227	16.108634
26.457531	856.842755	16.113651
26.466398	847.922906	16.118669
26.345789	858.244729	16.123687
26.387965	855.284794	16.128704
26.350891	839.460722	16.133722
26.162201	854.745910	16.138739
26.411235	854.292926	16.143757
26.413034	859.269569	16.148775
26.256834	855.294899	16.153792
26.855123	843.716568	16.158810
26.228040	852.162119	16.163827
26.626471	848.190491	16.168845
26.598054	848.898742	16.173863
26.521706	851.774657	16.178880
26.483789	849.340949	16.183898
26.216654	851.500069	16.188915
26.502595	849.642624	16.193933
26.385086	843.790784	16.198951
26.150484	854.041327	16.203968
26.345668	844.641047	16.208986
26.415745	868.266416	16.214003
26.613110	865.443766	16.219021
26.801821	875.734854	16.224039
26.720724	881.661403	16.229056
26.993501	869.144877	16.234074
26.795353	865.924355	16.239091
27.109732	868.161983	16.244109
26.995814	870.258731	16.249127
27.031445	865.100386	16.254144
26.898583	859.875065	16.259162
27.070194	866.427051	16.264179
27.053867	868.582438	16.269197
27.265436	871.656733	16.274215
26.984427	870.924998	16.279232
27.277604	863.205636	16.284250
27.079024	868.289867	16.289267
27.439910	867.648686	16.294285
27.120191	862.446431	16.299303
27.097377	865.184356	16.304320
27.347142	859.800803	16.309338
27.000520	864.118249	16.314355
26.997189	862.202800	16.319373
26.861405	864.275610	16.324391
26.770510	866.875604	16.329408
27.089984	859.799887	16.334426
27.365548	880.361096	16.339443
27.688570	880.026562	16.344461
27.662420	881.123790	16.349479
27.595603	872.108196	16.354496
27.737580	862.669474	16.359514
27.596685	859.413490	16.364531
27.645544	856.210728	16.369549
27.921462	859.341291	16.374567
27.639996	858.344292	16.379584
27.545570	851.947316	16.384602
27.722658	849.882317	16.389619
27.533833	852.937083	16.394637
27.565262	855.102670	16.399655
27.714608	863.828699	16.404672
27.950602	862.414539	16.409690
27.703864	861.720434	16.414707
28.104549	862.946187	16.419725
27.648748	858.937663	16.424743
27.851234	865.573903	16.429760
27.882885	878.240876	16.434778
27.754972	882.095363	16.439795
27.953306	884.182139	16.444813
28.022844	877.064733	16.449831
28.005731	894.119095	16.454848
28.371157	875.762716	16.459866
28.320213	880.952813	16.464883
27.901500	881.002501	16.469901
28.304599	873.153128	16.474919
28.295330	877.683602	16.479936
27.963076	874.892742	16.484954
28.222555	880.616055	16.489971
28.294020	879.505500	16.494989
28.459808	878.622621	16.500007
27.945253	891.583580	16.505024
28.149400	872.750392	16.510042
28.354481	885.019382	16.515059
28.227954	880.077636	16.520077
28.212062	882.530182	16.525095
28.349075	889.221365	16.530112
28.609824	881.862463	16.535130
28.330651	881.214277	16.540147
27.942572	881.712806	16.545165
28.340778	884.145207	16.550183
28.586431	887.864222	16.555200
28.603216	873.003195	16.560218
28.412511	892.933002	16.565235
28.545929	894.550631	16.570253
28.930999	908.280706	16.575271
29.009474	896.867931	16.580288
28.805563	883.565014	16.585306
28.811125	890.492125	16.590323
28.746350	882.208040	16.595341
28.934437	881.651374	16.600359
28.444749	882.756854	16.605376
28.758419	887.029932	16.610394
28.770744	903.475523	16.615411
28.766240	900.150099	16.620429
29.029569	900.997437	16.625447
28.905437	909.004246	16.630464
28.989867	897.813701	16.635482
29.120096	899.163369	16.640499
29.157358	909.386649	16.645517
29.043865	901.273998	16.650535
28.876133	902.652925	16.655552
29.359718	894.641403	16.660570
29.296566	899.836678	16.665587
28.993907	897.791663	16.670605
29.057431	897.873307	16.675623
29.223988	903.797438	16.680640
29.209609	895.985685	16.685658
29.167516	894.778978	16.690675
29.079597	896.694267	16.695693
29.172733	894.628596	16.700711
28.843848	919.248797	16.705728
29.731292	916.535091	16.710746
29.749246	925.408889	16.715763
29.317315	926.989824	16.720781
29.950969	926.879826	16.725799
29.898774	922.169448	16.730816
29.644200	904.970368	16.735834
29.555239	899.218105	16.740851
29.745201	904.749011	16.745869
29.618674	908.094245	16.750887
29.662669	914.493376	16.755904
30.176994	915.699529	16.760922
29.963171	917.731332	16.765939
29.468971	896.976841	16.770957
29.697430	908.894752	16.775975
29.563833	916.258676	16.780992
29.729069	921.315359	16.786010
30.071118	915.111033	16.791027
30.056655	921.136794	16.796045
30.357336	915.127498	16.801063
30.256563	915.794980	16.806080
30.505258	918.414734	16.811098
30.140964	902.314480	16.816115
30.323466	895.876357	16.821133
29.342264	890.909992	16.826151
29.755191	904.835048	16.831168
29.988876	923.502950	16.836186
30.263059	928.629387	16.841203
30.533988	928.167658	16.846221
30.430116	921.734031	16.851239
30.043252	928.036014	16.856256
30.188294	920.651373	16.861274
30.261086	917.848947	16.866291
30.162815	918.551839	16.871309
30.206994	916.702136	16.876327
30.120997	936.427268	16.881344
30.098034	919.942541	16.886362
30.365900	928.902907	16.891379
30.293114	932.436482	16.896397
30.662171	941.742288	16.901415
30.485116	946.087188	16.906432
30.639118	948.719083	16.911450
30.760204	939.695171	16.916467
30.722233	943.399354	16.921485
30.888142	942.974698	16.926503
30.771826	944.875799	16.931520
30.936530	942.132555	16.936538
30.811703	933.973735	16.941555
30.452542	946.120857	16.946573
30.585154	948.325606	16.951591
31.083895	939.672605	16.956608
31.102736	936.045290	16.961626
31.205879	939.860746	16.966643
31.070413	945.271543	16.971661
31.503383	935.850338	16.976679
31.081418	924.236955	16.981696
30.790815	922.410402	16.986714
31.347622	920.467156	16.991731
31.049251	931.366467	16.996749
31.392412	932.089176	17.001767
31.462674	927.382928	17.006784
31.429595	911.879364	17.011802
30.989247	902.615775	17.016819
31.160123	920.169721	17.021837
31.363313	924.789827	17.026855
31.479312	937.181871	17.031872
31.429708	932.689948	17.036890
31.183168	923.716681	17.041907
31.338074	939.008442	17.046925
31.361490	930.041651	17.051943
31.267614	936.517160	17.056960
31.579245	936.237265	17.061978
31.616498	927.346527	17.066995
31.165445	940.996977	17.072013
31.433148	931.396851	17.077031
31.368510	943.624725	17.082048
31.284390	944.245358	17.087066
31.349799	938.284852	17.092083
31.545708	959.036906	17.097101
32.066802	957.647575	17.102119
32.219686	963.889333	17.107136
32.200759	948.621566	17.112154
32.016870	934.945622	17.117171
31.604450	930.228355	17.122189
31.947686	928.927134	17.127207
32.121187	946.651140	17.132224
31.993983	951.337770	17.137242
32.291473	935.503082	17.142259
32.205737	937.934132	17.147277
32.159141	924.739376	17.152295
31.654827	918.660624	17.157312
31.727678	936.492617	17.162330
32.198596	935.888724	17.167347
32.043755	963.322560	17.172365
32.279699	954.341823	17.177383
32.585512	952.994831	17.182400
32.352306	954.742855	17.187418
32.533205	946.273182	17.192435
32.173308	950.921180	17.197453
32.398331	948.287233	17.202471
32.144633	952.707421	17.207488
32.233910	951.390772	17.212506
32.828464	949.328679	17.217523
31.975921	955.989657	17.222541
32.491057	938.763085	17.227559
32.719308	947.815451	17.232576
32.295839	953.779427	17.237594
32.685449	940.558884	17.242611
32.234691	949.932333	17.247629
32.768811	958.776980	17.252647
32.872802	976.293642	17.257664
32.840891	975.597817	17.262682
32.912450	971.159832	17.267699
32.759771	980.650078	17.272717
33.219223	973.194456	17.277735
33.021986	958.697903	17.282752
32.541729	946.453633	17.287770
32.973811	954.641583	17.292787
32.936562	969.048699	17.297805
33.304137	964.667603	17.302823
33.194622	972.520850	17.307840
33.340481	966.452528	17.312858
33.416155	962.474080	17.317875
33.119944	958.937900	17.322893
33.504860	949.962419	17.327911
33.161220	939.859998	17.332928
33.009407	942.618510	17.337946
33.372561	958.008086	17.342963
33.375935	965.699731	17.347981
33.465227	973.288969	17.352999
33.282148	970.496618	17.358016
33.473497	976.163928	17.363034
33.702082	965.584081	17.368051
33.373007	966.249606	17.373069
33.160219	966.388812	17.378087
33.306533	967.920066	17.383104
33.506942	975.481851	17.388122
33.430964	965.359897	17.393139
33.204067	971.253931	17.398157
33.454068	963.931808	17.403175
33.308377	973.354754	17.408192
33.496691	984.258945	17.413210
33.695565	994.465757	17.418227
33.559127	997.839029	17.423245
34.099571	996.471686	17.428263
34.189554	993.767970	17.433280
34.055968	995.051491	17.438298
34.042334	994.399881	17.443315
33.602617	997.878485	17.448333
34.076612	987.519395	17.453351
34.007214	992.293706	17.458368
33.830978	990.610799	17.463386
34.187176	990.717995	17.468403
33.806508	993.995884	17.473421
33.848797	992.459069	17.478439
34.321109	992.941115	17.483456
34.260606	984.875943	17.488474
34.397182	983.947505	17.493491
34.252980	987.924395	17.498509
34.360900	997.896281	17.503527
34.689763	999.889022	17.508544
34.492261	1005.558920	17.513562
34.679603	994.344179	17.518579
34.545342	992.824787	17.523597
34.314090	992.882408	17.528615
34.631326	986.986874	17.533632
34.549944	994.933502	17.538650
34.965399	1000.905037	17.543667
34.658080	984.225209	17.548685
34.461311	987.509259	17.553703
34.854797	999.029460	17.558720
34.518167	1008.268303	17.563738
35.102313	1007.961000	17.568755
34.902832	1014.076879	17.573773
35.047360	1002.377117	17.578791
34.880104	997.287753	17.583808
34.820459	990.152710	17.588826
35.033599	992.457119	17.593843
35.093229	1009.600472	17.598861
34.937967	1006.104326	17.603879
35.116427	1007.073593	17.608896
34.796596	1008.075762	17.613914
35.298768	1002.533442	17.618931
35.095484	1012.499782	17.623949
35.128590	1007.342595	17.628967
35.124461	1005.361909	17.633984
35.139327	1008.075906	17.639002
35.387453	1006.147935	17.644019
35.022891	1003.827735	17.649037
35.060728	1006.169046	17.654055
35.448721	1002.104230	17.659072
34.930126	1001.706696	17.664090
34.981296	1003.932418	17.669107
35.433220	1025.106717	17.674125
35.522028	1036.299457	17.679143
35.701530	1022.938445	17.684160
35.723767	1034.889026	17.689178
35.785199	1025.709200	17.694195
35.767786	1033.335426	17.699213
35.517907	1031.006074	17.704231
35.854848	1023.312850	17.709248
35.670775	1032.863836	17.714266
35.704557	1023.495684	17.719283
35.753781	1027.394889	17.724301
35.772289	1025.865158	17.729319
35.802716	1024.767687	17.734336
35.593194	1028.880988	17.739354
35.845800	1029.732472	17.744371
36.015190	1035.836492	17.749389
36.261936	1053.856748	17.754407
36.743706	1045.119889	17.759424
36.181165	1038.929868	17.764442
36.245317	1024.356116	17.769459
36.131231	1024.784478	17.774477
36.285573	1020.533945	17.779495
36.444050	1015.755586	17.784512
36.535336	1025.425532	17.789530
36.614594	1016.976587	17.794547
36.587768	1021.647013	17.799565
36.455301	1013.898452	17.804583
36.765381	1020.127197	17.809600
36.710861	1022.761350	17.814618
36.793998	1014.811349	17.819635
36.674053	1013.595476	17.824653
36.715129	1018.681804	17.829671
36.714591	1015.722218	17.834688
36.464969	1025.754111	17.839706
36.488562	1023.535771	17.844723
36.603628	1021.725103	17.849741
36.520658	1027.294946	17.854759
36.934325	1031.199947	17.859776
36.835740	1043.850040	17.864794
37.107959	1045.912007	17.869811
36.818509	1043.917538	17.874829
36.556266	1045.971942	17.879847
37.103219	1044.322427	17.884864
36.882848	1046.059280	17.889882
36.758337	1045.385871	17.894899
37.064869	1049.020832	17.899917
36.893494	1049.850398	17.904935
36.943007	1036.414445	17.909952
36.565836	1041.397993	17.914970
37.076900	1060.329964	17.919987
37.094804	1064.498133	17.925005
37.309174	1075.143754	17.930023
37.740013	1069.613222	17.935040
37.551382	1072.994758	17.940058
37.631399	1071.685537	17.945075
37.983063	1060.502593	17.950093
37.588731	1056.412581	17.955111
38.158852	1035.605682	17.960128
37.695913	1039.820393	17.965146
37.633122	1031.393386	17.970163
37.647048	1031.706068	17.975181
37.668551	1033.927652	17.980199
37.759899	1033.622422	17.985216
37.644053	1037.036385	17.990234
37.698574	1029.084028	17.995251
37.523467	1034.292374	18.000269
37.968406	1051.395595	18.005287
38.148844	1053.516853	18.010304
37.940965	1060.237660	18.015322
37.818025	1059.414389	18.020339
38.160039	1062.534444	18.025357
38.051347	1069.454177	18.030375
37.852637	1057.181310	18.035392
37.879487	1064.373468	18.040410
38.022453	1065.246257	18.045427
37.946703	1060.193687	18.050445
38.197893	1062.238273	18.055463
38.370231	1052.084594	18.060480
38.253062	1064.514955	18.065498
38.120554	1060.335529	18.070515
38.033814	1067.789400	18.075533
38.433053	1076.663929	18.080551
38.572394	1080.478938	18.085568
38.366158	1079.288371	18.090586
38.506238	1079.114042	18.095603
38.860081	1080.572364	18.100621
38.338725	1079.561135	18.105639
38.781101	1072.176007	18.110656
38.862921	1080.570047	18.115674
38.895005	1076.643667	18.120691
39.161482	1070.832487	18.125709
38.617858	1092.081566	18.130727
38.754191	1079.093388	18.135744
38.747241	1088.719406	18.140762
38.850406	1082.625039	18.145779
39.307192	1069.987729	18.150797
39.105600	1085.989821	18.155815
39.098406	1075.899316	18.160832
39.239501	1087.259020	18.165850
39.038985	1078.039074	18.170867
39.362934	1080.159407	18.175885
38.986027	1082.820574	18.180903
38.873403	1077.525689	18.185920
38.813071	1092.152481	18.190938
39.563534	1106.089151	18.195955
39.633546	1113.244659	18.200973
39.499591	1114.762100	18.205991
39.824429	1109.478625	18.211008
39.764722	1106.579210	18.216026
39.709786	1093.264042	18.221043
39.711395	1083.226010	18.226061
39.410969	1080.956592	18.231079
39.347834	1075.918857	18.236096
39.603821	1088.553188	18.241114
39.416857	1095.782732	18.246131
39.797817	1098.881386	18.251149
39.638099	1105.956035	18.256167
39.943844	1098.995472	18.261184
39.888116	1097.401257	18.266202
39.938576	1107.398869	18.271219
39.922065	1101.221951	18.276237
39.948268	1104.613590	18.281255
40.141217	1110.419656	18.286272
39.868369	1103.985192	18.291290
39.856733	1101.581343	18.296307
40.344724	1093.954803	18.301325
40.038445	1110.754145	18.306343
40.306789	1097.972038	18.311360
39.797046	1108.052959	18.316378
40.095256	1097.205205	18.321395
39.880456	1104.205119	18.326413
39.962617	1116.226940	18.331431
40.488404	1118.925647	18.336448
40.384931	1128.775539	18.341466
40.476773	1126.448644	18.346483
40.552900	1114.775476	18.351501
40.561545	1128.828698	18.356519
40.663021	1111.267294	18.361536
40.811413	1119.223969	18.366554
40.763701	1116.323747	18.371571
40.747092	1119.541776	18.376589
40.991319	1121.302887	18.381607
41.240443	1115.965019	18.386624
40.945702	1120.062535	18.391642
40.742155	1115.431880	18.396659
41.114494	1105.771409	18.401677
40.916633	1114.205477	18.406695
41.226446	1113.199924	18.411712
41.088608	1117.410036	18.416730
40.959627	1122.548965	18.421747
41.290409	1116.871210	18.426765
41.224009	1113.591814	18.431783
41.461466	1113.496239	18.436800
41.194758	1113.697128	18.441818
41.092009	1110.334777	18.446835
41.305445	1109.331797	18.451853
40.938421	1115.504589	18.456871
41.282919	1131.769051	18.461888
41.661947	1140.350911	18.466906
41.813899	1143.554814	18.471923
41.987454	1135.386637	18.476941
41.939496	1138.278769	18.481959
42.115006	1115.034829	18.486976
41.878567	1107.631771	18.491994
42.159055	1098.134146	18.497011
42.059078	1100.454197	18.502029
41.693656	1104.836236	18.507047
41.758958	1093.941619	18.512064
41.916098	1103.311746	18.517082
41.905579	1097.940106	18.522099
41.964925	1091.287264	18.527117
41.760721	1098.809023	18.532135
42.099193	1099.656529	18.537152
42.045512	1095.596713	18.542170
42.112243	1107.406130	18.547187
42.174280	1104.328296	18.552205
42.179983	1130.490223	18.557223
42.196361	1128.682498	18.562240
42.736796	1135.979801	18.567258
42.281097	1132.712106	18.572275
42.041310	1130.381855	18.577293
41.792450	1130.001069	18.582311
42.389356	1125.383144	18.587328
42.563279	1118.253067	18.592346
42.106770	1129.286177	18.597363
42.390029	1128.343285	18.602381
42.514330	1128.487699	18.607399
42.344082	1133.979121	18.612416
42.887779	1142.709696	18.617434
42.627462	1145.021265	18.622451
42.951629	1154.473211	18.627469
42.820534	1165.681591	18.632487
42.720390	1154.545043	18.637504
43.218979	1151.916158	18.642522
43.036236	1159.758398	18.647539
43.303408	1145.570193	18.652557
43.144504	1145.987869	18.657575
43.239324	1152.221996	18.662592
43.329834	1144.901001	18.667610
42.841543	1140.639129	18.672627
43.319643	1141.315886	18.677645
43.603666	1144.638860	18.682663
43.118042	1143.029604	18.687680
43.349120	1136.980568	18.692698
43.306611	1147.239261	18.697715
43.425103	1133.868177	18.702733
43.076615	1150.209607	18.707751
43.522063	1151.898036	18.712768
43.411719	1146.012612	18.717786
43.267180	1141.242656	18.722803
43.313562	1143.073929	18.727821
43.416194	1156.602970	18.732839
43.175048	1161.749067	18.737856
43.735813	1169.174512	18.742874
43.436610	1177.793893	18.747891
43.890026	1174.426445	18.752909
43.918169	1186.038381	18.757927
43.516671	1182.582966	18.762944
43.688709	1182.774986	18.767962
43.796628	1191.800571	18.772979
44.373944	1193.599844	18.777997
44.543206	1205.012449	18.783015
44.135052	1198.249572	18.788032
44.601731	1198.701065	18.793050
44.326246	1187.961231	18.798067
44.657369	1178.270533	18.803085
44.835201	1165.858856	18.808103
44.503331	1163.393851	18.813120
44.511520	1165.703483	18.818138
44.495790	1163.443998	18.823155
44.695523	1161.849208	18.828173
44.432172	1158.869333	18.833191
44.391758	1160.850408	18.838208
44.774890	1153.342380	18.843226
44.221795	1168.190594	18.848243
44.615649	1173.449262	18.853261
44.956846	1180.060308	18.858279
45.107574	1181.934149	18.863296
45.304724	1190.629222	18.868314
44.931322	1185.409760	18.873331
45.088837	1183.377091	18.878349
44.899844	1190.801497	18.883367
44.856898	1188.650055	18.888384
45.126309	1180.638812	18.893402
44.876613	1185.663108	18.898419
45.264022	1178.052394	18.903437
45.062414	1173.982406	18.908455
45.248620	1187.781485	18.913472
45.348418	1185.839079	18.918490
44.985892	1182.952389	18.923507
45.464264	1174.617976	18.928525
45.387981	1177.700233	18.933543
45.165316	1180.666181	18.938560
45.066396	1190.629528	18.943578
45.088677	1208.253286	18.948595
45.588975	1204.958776	18.953613
45.645661	1208.396963	18.958631
45.294911	1216.042253	18.963648
45.376084	1207.884610	18.968666
45.329078	1211.882864	18.973683
45.763093	1223.252040	18.978701
46.162759	1227.681442	18.983719
46.631135	1233.221484	18.988736
46.058986	1206.467449	18.993754
46.046182	1205.833408	18.998771
46.257229	1198.893992	19.003789
46.044159	1196.885281	19.008807
46.085063	1207.655382	19.013824
46.320857	1196.699000	19.018842
46.095559	1210.347738	19.023859
46.199147	1212.228207	19.028877
46.498130	1216.167206	19.033895
46.551682	1222.123164	19.038912
47.015925	1219.260985	19.043930
46.403597	1221.179289	19.048947
46.678135	1217.838300	19.053965
46.518338	1219.922612	19.058983
46.550523	1219.353561	19.064000
46.825031	1218.610532	19.069018
46.871963	1217.377641	19.074035
47.116582	1215.370308	19.079053
47.156644	1223.591424	19.084071
46.811374	1211.770247	19.089088
46.872061	1202.769174	19.094106
46.642793	1221.475511	19.099123
46.917496	1214.696803	19.104141
47.001066	1222.358369	19.109159
46.802462	1228.719455	19.114176
47.305582	1217.967212	19.119194
46.939023	1224.691529	19.124211
46.467891	1213.544321	19.129229
46.984279	1226.688389	19.134247
47.011926	1251.487872	19.139264
47.345402	1252.268501	19.144282
47.239776	1256.765829	19.149299
47.199662	1258.611044	19.154317
47.293348	1250.308004	19.159335
47.405258	1257.434988	19.164352
47.775945	1238.502129	19.169370
47.615291	1242.521570	19.174387
47.836259	1238.409155	19.179405
47.842501	1236.655849	19.184423
47.207213	1240.197989	19.189440
47.901336	1247.729341	19.194458
47.760466	1262.583403	19.199475
47.841049	1264.568472	19.204493
48.425281	1275.359286	19.209511
47.994731	1270.311852	19.214528
48.341620	1273.409884	19.219546
48.496116	1276.912205	19.224563
48.424444	1262.805588	19.229581
48.669995	1266.403456	19.234599
48.394464	1250.622775	19.239616
48.821029	1241.725661	19.244634
48.301175	1249.232436	19.249651
48.165024	1234.935738	19.254669
48.333354	1239.795957	19.259687
48.026395	1234.967434	19.264704
48.388974	1237.568782	19.269722
48.776200	1254.160541	19.274739
48.781776	1256.285584	19.279757
48.913583	1250.803714	19.284775
48.734563	1251.082602	19.289792
48.947105	1253.361560	19.294810
48.673189	1250.755846	19.299827
48.769981	1256.877881	19.304845
49.417842	1257.354099	19.309863
48.996359	1258.332171	19.314880
48.979436	1240.661880	19.319898
48.761965	1250.737412	19.324915
48.643581	1260.216245	19.329933
49.286362	1248.300337	19.334951
49.185808	1257.227805	19.339968
48.996087	1248.213839	19.344986
49.315968	1251.424210	19.350003
48.934186	1246.773028	19.355021
49.311451	1258.052810	19.360039
49.433766	1273.967213	19.365056
49.575825	1279.097929	19.370074
49.525296	1280.461419	19.375091
49.712776	1277.034048	19.380109
49.867141	1280.099001	19.385127
49.626269	1284.179372	19.390144
49.990415	1278.991297	19.395162
50.034681	1273.828237	19.400179
50.157868	1278.538072	19.405197
49.611735	1276.754572	19.410215
49.548559	1279.744130	19.415232
49.633239	1283.492651	19.420250
49.868246	1270.867099	19.425267
49.697779	1284.330056	19.430285
50.036645	1286.198743	19.435303
49.791695	1306.021530	19.440320
50.080033	1305.056134	19.445338
49.969015	1305.923748	19.450355
50.033189	1314.917280	19.455373
50.502364	1303.958793	19.460391
50.367212	1307.914975	19.465408
50.643168	1300.523045	19.470426
50.528910	1308.849677	19.475443
50.785381	1319.502276	19.480461
50.897689	1332.406262	19.485479
50.760791	1333.267533	19.490496
51.065847	1325.468026	19.495514
50.980623	1307.340475	19.500531
51.014828	1300.523206	19.505549
50.793136	1295.626610	19.510567
50.573264	1308.378101	19.515584
50.996556	1321.667190	19.520602
51.041364	1326.843157	19.525619
51.138317	1329.215280	19.530637
51.425797	1319.031338	19.535655
50.950370	1330.314960	19.540672
51.255744	1324.264574	19.545690
50.973994	1317.580318	19.550707
51.212351	1324.751750	19.555725
51.225243	1327.907458	19.560743
51.160057	1324.376246	19.565760
51.249084	1330.787385	19.570778
51.658057	1345.048528	19.575795
51.730518	1345.632227	19.580813
51.822130	1340.155013	19.585831
52.025439	1341.762299	19.590848
51.862239	1342.617690	19.595866
52.197134	1336.799414	19.600883
52.004984	1330.502670	19.605901
52.055381	1313.501844	19.610919
51.869336	1308.158801	19.615936
52.042014	1313.770274	19.620954
52.125062	1317.124201	19.625971
52.056836	1334.778837	19.630989
52.129069	1336.982223	19.636007
52.272256	1343.595812	19.641024
52.432436	1335.622654	19.646042
52.405857	1331.944894	19.651059
52.466954	1336.992580	19.656077
52.614144	1327.975537	19.661095
52.759489	1332.913999	19.666112
52.772468	1330.200140	19.671130
52.609158	1329.627234	19.676147
52.782653	1334.320489	19.681165
52.872665	1326.805401	19.686183
52.374542	1330.381934	19.691200
52.863156	1326.011799	19.696218
52.858324	1323.818989	19.701235
52.705002	1326.604982	19.706253
52.785216	1322.774899	19.711271
52.528817	1328.692063	19.716288
52.623793	1325.133938	19.721306
52.517360	1331.806175	19.726323
52.737350	1354.692917	19.731341
53.241492	1352.304808	19.736359
53.165246	1360.746825	19.741376
53.502612	1365.216898	19.746394
53.427891	1361.784105	19.751411
53.096245	1362.461093	19.756429
53.255615	1360.498171	19.761447
53.230450	1377.315428	19.766464
53.488347	1377.204264	19.771482
53.356136	1391.685763	19.776499
53.252168	1391.116022	19.781517
53.598877	1388.446106	19.786535
53.607154	1393.811212	19.791552
53.525545	1392.205897	19.796570
53.876752	1384.633360	19.801587
53.987700	1402.790286	19.806605
54.333528	1405.920805	19.811623
54.334657	1404.900598	19.816640
54.507918	1387.313216	19.821658
54.374942	1385.415625	19.826675
54.059385	1383.075440	19.831693
54.123908	1375.280695	19.836711
54.169526	1392.303961	19.841728
54.137744	1412.769923	19.846746
54.243071	1395.442200	19.851763
54.440733	1413.263134	19.856781
54.693496	1401.803413	19.861799
54.644315	1410.050428	19.866816
54.806329	1407.910687	19.871834
55.065628	1408.229993	19.876851
54.503196	1409.114876	19.881869
55.036691	1407.856919	19.886887
55.070734	1413.082728	19.891904
54.762336	1414.242474	19.896922
54.957419	1401.536026	19.901939
54.857906	1409.837436	19.906957
54.692010	1402.657985	19.911975
54.733856	1427.308551	19.916992
54.821555	1427.444462	19.922010
55.261166	1433.560198	19.927027
55.299776	1435.375077	19.932045
55.241133	1436.914724	19.937063
55.015843	1435.228866	19.942080
55.233124	1431.615427	19.947098
55.393565	1431.540872	19.952115
55.204752	1442.183033	19.957133
55.473154	1456.131733	19.962151
55.520061	1466.738819	19.967168
55.955796	1467.252531	19.972186
55.788925	1453.257564	19.977203
55.707688	1469.260595	19.982221
56.043949	1455.962624	19.987239
55.929220	1461.491425	19.992256
56.021630	1471.070128	19.997274
56.247819	1460.019483	20.002291
55.793035	1464.876647	20.007309
56.117519	1459.219496	20.012327
56.274727	1458.305330	20.017344
56.105873	1459.430557	20.022362
56.384929	1460.110761	20.027379
56.310048	1456.598053	20.032397
56.505104	1464.341672	20.037415
56.513133	1476.461480	20.042432
56.766638	1473.446751	20.047450
56.753835	1476.953196	20.052467
56.529977	1480.748521	20.057485
56.884942	1468.129718	20.062503
56.884365	1475.114012	20.067520
56.908201	1475.398685	20.072538
57.362413	1469.922410	20.077555
56.894669	1470.816028	20.082573
57.175502	1475.819503	20.087591
57.096047	1479.236198	20.092608
57.166852	1469.896685	20.097626
57.049265	1472.101205	20.102643
56.966461	1467.520136	20.107661
56.770798	1472.915099	20.112679
56.842571	1474.544573	20.117696
57.299923	1492.687950	20.122714
57.647396	1494.931217	20.127731
57.346634	1491.847236	20.132749
57.481536	1492.207218	20.137767
57.657417	1486.916784	20.142784
57.449305	1500.650726	20.147802
57.601714	1490.429589	20.152819
57.215733	1508.053571	20.157837
57.745624	1513.542586	20.162855
58.360144	1519.310108	20.167872
58.060532	1519.264481	20.172890
58.033543	1520.350869	20.177907
58.349650	1521.971782	20.182925
58.134379	1522.318092	20.187943
58.335557	1528.123742	20.192960
58.396859	1518.196409	20.197978
58.559656	1519.020273	20.202995
58.523845	1526.458451	20.208013
58.676658	1515.307713	20.213031
58.669996	1525.771742	20.218048
58.296376	1526.577337	20.223066
58.763217	1525.886701	20.228083
58.645874	1525.168383	20.233101
58.516189	1523.062358	20.238119
58.589665	1519.880580	20.243136
58.587354	1527.260850	20.248154
58.523781	1517.773087	20.253171
58.289829	1540.683691	20.258189
58.476680	1554.167246	20.263207
58.949256	1549.889468	20.268224
58.802288	1546.228834	20.273242
58.956907	1545.096197	20.278259
59.121983	1562.555772	20.283277
59.045669	1570.140834	20.288295
59.193063	1574.534156	20.293312
59.651903	1577.042853	20.298330
60.020822	1564.335441	20.303347
59.315537	1575.336828	20.308365
59.549844	1568.574497	20.313383
59.483405	1568.850104	20.318400
59.431187	1580.102021	20.323418
59.756183	1571.767204	20.328435
59.722001	1576.418935	20.333453
59.644722	1562.507460	20.338471
59.800748	1569.765472	20.343488
59.861559	1594.701745	20.348506
60.418390	1589.997410	20.353523
60.049565	1600.749405	20.358541
60.258273	1593.873193	20.363559
60.718761	1601.859938	20.368576
60.356252	1596.346408	20.373594
60.693463	1591.189068	20.378611
60.455180	1587.494725	20.383629
60.476184	1588.883799	20.388647
60.513098	1588.169464	20.393664
60.472710	1590.743894	20.398682
61.010090	1593.511635	20.403699
60.879432	1595.428968	20.408717
60.748281	1585.975187	20.413735
60.936308	1588.114555	20.418752
60.496434	1588.217742	20.423770
60.487066	1588.433899	20.428787
60.907534	1601.894169	20.433805
60.782639	1618.355367	20.438823
60.950850	1617.676378	20.443840
60.877742	1617.214509	20.448858
61.369246	1620.618983	20.453875
61.167402	1620.065831	20.458893
61.124751	1615.227677	20.463911
61.656697	1623.681341	20.468928
61.261661	1635.241634	20.473946
61.803236	1638.671680	20.478963
61.786422	1646.343777	20.483981
62.078985	1643.790265	20.488999
61.858398	1641.022898	20.494016
61.663617	1639.333540	20.499034
61.605846	1635.721896	20.504051
61.856880	1642.839408	20.509069
61.670234	1635.201474	20.514087
62.243385	1628.418841	20.519104
61.816157	1634.864797	20.524122
62.078033	1630.976607	20.529139
62.326052	1639.794613	20.534157
62.280070	1654.033339	20.539175
62.836133	1669.317278	20.544192
62.747043	1661.820658	20.549210
62.814316	1652.733589	20.554227
62.599525	1647.879832	20.559245
62.561471	1646.278696	20.564263
63.001382	1654.840922	20.569280
62.967924	1663.496885	20.574298
63.183686	1659.967898	20.579315
62.710511	1642.598677	20.584333
62.832753	1656.407979	20.589351
63.119573	1643.427089	20.594368
63.127625	1652.324204	20.599386
63.298441	1649.295574	20.604403
63.329184	1654.105082	20.609421
63.040927	1648.957978	20.614439
63.344612	1644.225463	20.619456
62.983046	1655.130230	20.624474
63.212376	1641.247445	20.629491
63.357280	1646.549466	20.634509
63.110371	1653.689193	20.639527
63.219644	1661.001446	20.644544
63.296855	1686.282001	20.649562
63.399874	1678.837030	20.654579
63.577215	1681.547077	20.659597
63.434620	1688.154589	20.664615
63.597416	1695.684767	20.669632
63.629059	1708.695730	20.674650
64.246394	1703.214807	20.679667
64.179880	1710.617212	20.684685
64.088317	1704.314291	20.689703
64.488447	1704.280364	20.694720
64.165007	1698.868989	20.699738
64.707702	1702.529573	20.704755
64.550822	1702.719368	20.709773
64.301082	1691.504446	20.714791
64.761067	1695.169274	20.719808
64.706094	1695.605583	20.724826
64.688677	1705.784112	20.729843
65.026840	1694.415548	20.734861
65.037481	1700.345330	20.739879
64.893800	1692.334505	20.744896
64.718022	1698.517593	20.749914
65.485255	1714.645354	20.754931
65.422878	1715.459662	20.759949
64.912139	1708.120628	20.764967
65.440051	1711.863190	20.769984
65.425101	1721.811400	20.775002
65.376990	1726.201308	20.780019
65.666325	1722.808551	20.785037
65.416290	1725.749999	20.790055
65.617343	1723.786430	20.795072
65.125093	1716.175827	20.800090
65.646187	1716.855732	20.805107
65.577868	1716.469052	20.810125
65.392302	1717.711238	20.815143
65.657909	1731.457105	20.820160
65.946972	1742.825863	20.825178
66.099426	1752.316845	20.830195
66.292297	1749.996752	20.835213
66.031075	1744.057734	20.840231
66.353774	1748.151213	20.845248
66.240716	1750.181005	20.850266
66.040771	1747.378705	20.855283
66.327634	1744.545410	20.860301
66.265676	1748.868327	20.865319
66.576266	1748.350404	20.870336
66.474830	1754.133802	20.875354
66.604253	1763.446320	20.880371
66.724697	1769.461492	20.885389
66.520021	1775.102935	20.890407
67.262251	1769.178473	20.895424
67.002188	1766.901481	20.900442
66.694255	1766.685576	20.905459
66.843561	1771.062496	20.910477
67.115895	1774.937941	20.915495
67.470497	1770.874915	20.920512
67.108329	1768.646717	20.925530
67.104964	1768.058335	20.930547
67.484670	1780.805035	20.935565
67.432134	1796.361521	20.940583
67.657074	1784.676203	20.945600
67.982077	1794.848883	20.950618
67.892863	1793.593213	20.955635
67.951836	1787.837385	20.960653
68.293845	1792.335161	20.965671
68.176767	1775.261558	20.970688
67.753092	1762.271435	20.975706
67.891286	1762.440328	20.980723
68.022922	1765.530401	20.985741
67.966922	1782.828009	20.990759
68.274944	1774.725029	20.995776
68.139153	1785.367307	21.000794
68.377572	1788.337342	21.005811
68.500852	1786.231523	21.010829
68.069986	1791.468687	21.015847
68.280090	1786.318550	21.020864
68.318108	1791.266661	21.025882
68.371738	1795.201946	21.030899
68.477957	1811.292009	21.035917
68.801858	1820.906222	21.040935
68.933524	1808.644985	21.045952
68.924630	1818.665089	21.050970
68.784469	1821.896240	21.055987
69.235278	1815.566465	21.061005
68.898625	1822.506953	21.066023
68.906815	1813.018545	21.071040
69.465745	1820.165870	21.076058
69.344750	1835.812472	21.081075
69.529774	1823.384514	21.086093
69.525112	1834.325983	21.091111
69.620220	1824.205060	21.096128
69.651398	1830.269681	21.101146
69.522769	1836.754469	21.106163
69.805231	1818.914658	21.111181
69.319585	1827.107781	21.116199
70.042251	1828.522829	21.121216
70.119533	1825.002561	21.126234
69.872609	1834.062470	21.131251
69.959284	1836.717084	21.136269
69.968130	1853.659936	21.141287
70.057054	1846.211313	21.146304
70.115616	1851.283602	21.151322
70.226584	1850.296755	21.156339
70.602932	1855.068396	21.161357
70.193738	1863.812666	21.166375
70.455285	1868.415914	21.171392
70.737610	1876.614982	21.176410
70.952812	1877.138847	21.181427
71.014849	1878.859740	21.186445
70.984609	1885.506213	21.191463
70.977399	1872.247434	21.196480
71.113050	1878.185720	21.201498
71.117151	1875.531898	21.206515
71.369453	1870.865697	21.211533
71.110187	1879.490663	21.216551
71.512110	1869.112216	21.221568
71.660515	1877.092509	21.226586
71.560629	1874.466141	21.231603
71.790394	1873.334818	21.236621
71.413865	1875.314942	21.241639
71.827855	1871.845607	21.246656
71.724417	1865.672147	21.251674
71.824810	1866.676444	21.256691
71.835337	1866.723167	21.261709
71.361438	1882.939671	21.266727
71.904361	1894.262965	21.271744
71.895114	1910.556110	21.276762
72.044933	1907.467520	21.281779
72.441047	1897.284507	21.286797
72.141636	1899.765652	21.291815
72.148386	1897.562181	21.296832
72.235423	1897.120246	21.301850
72.246221	1918.757400	21.306867
72.954393	1921.424877	21.311885
72.602490	1926.586412	21.316903
72.768961	1928.562466	21.321920
72.480397	1920.666064	21.326938
72.684367	1920.353588	21.331955
73.012029	1913.119740	21.336973
72.918528	1918.675110	21.341991
72.907887	1912.526818	21.347008
72.931242	1924.069233	21.352026
72.911744	1939.312907	21.357043
73.694212	1945.170109	21.362061
73.689581	1956.702615	21.367079
73.475223	1946.387965	21.372096
73.610887	1946.251368	21.377114
73.435885	1944.548464	21.382131
73.826736	1951.911086	21.387149
73.788199	1947.212700	21.392167
73.817416	1949.554007	21.397184
73.837574	1945.530562	21.402202
73.533556	1945.421881	21.407219
74.106152	1942.409743	21.412237
73.791508	1952.661269	21.417255
73.666901	1960.382078	21.422272
74.055604	1966.535985	21.427290
74.181529	1968.400644	21.432307
74.561990	1965.997491	21.437325
74.606298	1968.434729	21.442343
74.768745	1972.044949	21.447360
74.687701	1963.825577	21.452378
74.404356	1970.022252	21.457395
74.607888	1980.899825	21.462413
74.821934	1997.532869	21.467431
74.705343	2005.225995	21.472448
75.191314	1997.303678	21.477466
75.457107	2000.906637	21.482483
75.390291	1993.132541	21.487501
75.285621	1989.459287	21.492519
75.570860	1988.791615	21.497536
75.532688	1979.393460	21.502554
75.401916	1994.540256	21.507571
75.897330	1978.054009	21.512589
75.877244	1986.534312	21.517607
75.619332	1983.529751	21.522624
75.949654	1985.029855	21.527642
75.412493	1990.570517	21.532659
75.303117	1988.288227	21.537677
75.499224	2007.547926	21.542695
75.855949	2004.759713	21.547712
76.043947	2003.141979	21.552730
75.818011	2009.407512	21.557747
76.326169	2018.896851	21.562765
76.314064	2028.997546	21.567783
76.996268	2038.827381	21.572800
76.694154	2030.404807	21.577818
76.705741	2033.308901	21.582835
77.004515	2033.183487	21.587853
76.779151	2026.145091	21.592871
77.170387	2033.254138	21.597888
77.186719	2025.781621	21.602906
77.365235	2026.414324	21.607923
77.357845	2027.139227	21.612941
77.177739	2020.727605	21.617959
77.156305	2026.467543	21.622976
77.361949	2026.178017	21.627994
76.801919	2030.007874	21.633011
77.240264	2030.795987	21.638029
77.433540	2035.533427	21.643047
77.310026	2037.768929	21.648064
77.268883	2025.536133	21.653082
77.219839	2050.149587	21.658099
77.591016	2059.591552	21.663117
77.497851	2057.936898	21.668135
77.587590	2067.754607	21.673152
77.880553	2065.275766	21.678170
77.957976	2077.490462	21.683187
78.210111	2085.848974	21.688205
78.291051	2091.461353	21.693223
78.574720	2092.541228	21.698240
78.597667	2093.859945	21.703258
78.539571	2092.963675	21.708275
78.744408	2085.608347	21.713293
78.967972	2090.699067	21.718311
78.678670	2085.180324	21.723328
78.994283	2090.161312	21.728346
78.646825	2092.396104	21.733363
78.894641	2086.571103	21.738381
78.885124	2086.692407	21.743399
79.110301	2084.874410	21.748416
79.341540	2083.438884	21.753434
78.896919	2102.459896	21.758451
79.403593	2110.065234	21.763469
79.505876	2116.506001	21.768487
79.336791	2111.249637	21.773504
79.613416	2110.568820	21.778522
79.738839	2111.605210	21.783539
79.598643	2113.283627	21.788557
79.537486	2116.704125	21.793575
79.757935	2126.197859	21.798592
80.060984	2133.954250	21.803610
79.814664	2135.379365	21.808627
79.941880	2125.410022	21.813645
79.905324	2127.910675	21.818663
79.957577	2132.980952	21.823680
80.278667	2149.439345	21.828698
80.189041	2162.191624	21.833715
80.576852	2161.109706	21.838733
80.533449	2156.126622	21.843751
80.631892	2163.603115	21.848768
80.851062	2154.307132	21.853786
80.665861	2157.840306	21.858803
81.272769	2168.891390	21.863821
81.032674	2183.524564	21.868839
81.062362	2179.095530	21.873856
81.629855	2177.476365	21.878874
81.468525	2183.427324	21.883891
81.675022	2178.665069	21.888909
81.687468	2178.036651	21.893927
81.560554	2172.980771	21.898944
82.023425	2173.939247	21.903962
81.882611	2181.651825	21.908979
81.739326	2173.017831	21.913997
82.055674	2175.299427	21.919015
81.934781	2184.081970	21.924032
82.202788	2172.546717	21.929050
82.030527	2177.200623	21.934067
81.921152	2175.546278	21.939085
82.217717	2174.317651	21.944103
82.055931	2171.073508	21.949120
82.274460	2183.161772	21.954138
82.228973	2195.048080	21.959155
82.221378	2193.532005	21.964173
82.291541	2196.022874	21.969191
82.087477	2205.173149	21.974208
82.609828	2226.352399	21.979226
82.568063	2228.774007	21.984243
82.354925	2228.711302	21.989261
82.957363	2229.959676	21.994279
82.480779	2238.397978	21.999296
83.245453	2248.004837	22.004314
83.022752	2248.079153	22.009331
83.517898	2249.253952	22.014349
83.537675	2248.997559	22.019367
83.573079	2245.475073	22.024384
83.932984	2239.808235	22.029402
83.828701	2252.123628	22.034419
83.875932	2242.799760	22.039437
84.523608	2245.993079	22.044455
84.255973	2250.046634	22.049472
84.395595	2242.969362	22.054490
84.300583	2244.107616	22.059507
84.433052	2240.214717	22.064525
84.466453	2246.744504	22.069543
84.134475	2242.408405	22.074560
84.426595	2241.223818	22.079578
84.340594	2257.411132	22.084595
84.877998	2260.576648	22.089613
84.915388	2269.673204	22.094631
84.905279	2265.905877	22.099648
85.049083	2271.946906	22.104666
84.865992	2271.002026	22.109683
84.851446	2266.304297	22.114701
85.051199	2261.241941	22.119719
84.563449	2269.049013	22.124736
85.108249	2281.740051	22.129754
85.155812	2296.470197	22.134771
85.027222	2299.371170	22.139789
85.503743	2292.418419	22.144807
85.269898	2308.097172	22.149824
85.451246	2305.728904	22.154842
85.584306	2330.281940	22.159859
85.696488	2326.513644	22.164877
86.267733	2324.654858	22.169895
85.923111	2329.585782	22.174912
86.449673	2328.458834	22.179930
86.612339	2342.597895	22.184947
86.440228	2345.423401	22.189965
86.816066	2345.921082	22.194983
86.577794	2347.575209	22.200000
86.983887	2342.097152	22.205018
86.912153	2343.681577	22.210035
86.952603	2344.314711	22.215053
86.970079	2335.107530	22.220071
86.857502	2351.695816	22.225088
86.942601	2327.731536	22.230106
87.155864	2341.111006	22.235123
87.285721	2340.861584	22.240141
87.220291	2336.082884	22.245159
87.101430	2337.634558	22.250176
87.460126	2347.843366	22.255194
87.689099	2363.890055	22.260211
87.363151	2368.586786	22.265229
87.714130	2374.223852	22.270247
87.511554	2370.585221	22.275264
87.933756	2363.982786	22.280282
87.932579	2372.196771	22.285299
87.825182	2364.669377	22.290317
88.179477	2383.780119	22.295335
87.870746	2388.541332	22.300352
87.981503	2397.457303	22.305370
88.238464	2390.554641	22.310387
88.309702	2383.128770	22.315405
88.749659	2399.698070	22.320423
89.167207	2408.761687	22.325440
89.033326	2407.237759	22.330458
89.378985	2398.297085	22.335475
89.075466	2388.459522	22.340493
89.106683	2370.233494	22.345511
88.959210	2379.417023	22.350528
89.220239	2389.951885	22.355546
89.595225	2395.894840	22.360563
89.585844	2409.522659	22.365581
89.623727	2408.623866	22.370599
89.598174	2414.225251	22.375616
89.408525	2395.142413	22.380634
89.675037	2394.501844	22.385651
89.855335	2394.048785	22.390669
90.044529	2393.195022	22.395687
89.826335	2406.837725	22.400704
90.089591	2404.432652	22.405722
89.909240	2424.841470	22.410739
90.074630	2429.118271	22.415757
90.532022	2424.060847	22.420775
90.411584	2424.171777	22.425792
90.243205	2421.018441	22.430810
90.342245	2428.874903	22.435827
90.474865	2456.014950	22.440845
90.880040	2447.794352	22.445863
91.145553	2456.005173	22.450880
91.228502	2446.782755	22.455898
91.642368	2446.446543	22.460915
91.274721	2448.614645	22.465933
91.449893	2451.148408	22.470951
91.338009	2452.011109	22.475968
91.726152	2448.232529	22.480986
91.612315	2443.762613	22.486003
91.805052	2451.895320	22.491021
91.701943	2439.142904	22.496039
91.422590	2459.019312	22.501056
91.754996	2465.381964	22.506074
92.152315	2477.682206	22.511091
91.842351	2477.281968	22.516109
92.151836	2479.466710	22.521127
92.117595	2476.862837	22.526144
91.908301	2485.946422	22.531162
92.057513	2504.215238	22.536179
92.337718	2517.276674	22.541197
92.570943	2504.248822	22.546215
92.583018	2516.940456	22.551232
92.905119	2525.206122	22.556250
92.982680	2527.976544	22.561267
93.044656	2532.672486	22.566285
92.978938	2533.429905	22.571303
92.852247	2532.807185	22.576320
93.458148	2521.849230	22.581338
93.824065	2527.835079	22.586355
93.425102	2532.475046	22.591373
93.237264	2531.054138	22.596391
93.307441	2551.070836	22.601408
93.339824	2558.825794	22.606426
93.939120	2556.922966	22.611443
93.477870	2546.546032	22.616461
94.113624	2563.714227	22.621479
94.301865	2571.965465	22.626496
94.358184	2575.985153	22.631514
94.824940	2576.850095	22.636531
94.707123	2573.941914	22.641549
94.658783	2575.157507	22.646567
94.427958	2570.296664	22.651584
94.967444	2577.692854	22.656602
95.119199	2570.106705	22.661619
95.071311	2577.654478	22.666637
95.149626	2566.844475	22.671655
95.331423	2568.914142	22.676672
94.935536	2568.570256	22.681690
94.990498	2568.904917	22.686707
94.921556	2583.795577	22.691725
94.987278	2593.023466	22.696743
94.968821	2612.109585	22.701760
95.171435	2604.325616	22.706778
95.597678	2613.635962	22.711795
95.933717	2630.771959	22.716813
96.056754	2620.453365	22.721831
95.925381	2629.154030	22.726848
95.889081	2626.479209	22.731866
96.167410	2619.748116	22.736883
96.437521	2627.703528	22.741901
96.292835	2613.518001	22.746919
96.490120	2628.480775	22.751936
96.452267	2644.424284	22.756954
96.516495	2651.771236	22.761971
96.680351	2659.658424	22.766989
97.239881	2646.902040	22.772007
96.570030	2651.819977	22.777024
96.899536	2650.952420	22.782042
97.253776	2656.303205	22.787059
97.306130	2670.636036	22.792077
97.682518	2669.381558	22.797095
97.891898	2666.658967	22.802112
97.673663	2669.505948	22.807130
97.541221	2667.224620	22.812147
97.794301	2666.382708	22.817165
98.099466	2660.618083	22.822183
98.132418	2661.452485	22.827200
97.789667	2665.107532	22.832218
98.065297	2666.458089	22.837235
97.955945	2690.267921	22.842253
98.341722	2692.170360	22.847271
98.605030	2697.201940	22.852288
98.544896	2696.832384	22.857306
98.549118	2693.516155	22.862323
98.392138	2699.231141	22.867341
98.737234	2718.760382	22.872359
99.145201	2727.868690	22.877376
98.842853	2731.537931	22.882394
99.284770	2719.187995	22.887411
99.414946	2720.061819	22.892429
99.640005	2715.435708	22.897447
99.690753	2720.561942	22.902464
99.357857	2715.977812	22.907482
99.156900	2719.751531	22.912499
99.546596	2742.351576	22.917517
99.921754	2743.924655	22.922535
100.322978	2743.160975	22.927552
99.989929	2759.218047	22.932570
100.097821	2746.973002	22.937587
100.123459	2752.829831	22.942605
100.280269	2749.870637	22.947623
100.386388	2768.538657	22.952640
100.427145	2774.611904	22.957658
100.806062	2772.405752	22.962675
100.499844	2785.124316	22.967693
100.589301	2775.934092	22.972711
100.806133	2782.020713	22.977728
100.616465	2793.564787	22.982746
101.152622	2804.760336	22.987763
101.582591	2806.853519	22.992781
101.579810	2802.667497	22.997799
101.834448	2804.736161	23.002816
101.511110	2800.653609	23.007834
101.626961	2790.384521	23.012851
101.686024	2797.426863	23.017869
101.825225	2799.142171	23.022887
101.960075	2801.391308	23.027904
101.582710	2795.125419	23.032922
101.868110	2812.460172	23.037939
101.882636	2823.513342	23.042957
102.213686	2826.061914	23.047975
102.352591	2826.631520	23.052992
102.397981	2829.514023	23.058010
102.702184	2836.700849	23.063027
102.641170	2851.216408	23.068045
102.912620	2846.952291	23.073063
102.985603	2854.114017	23.078080
102.736975	2851.171138	23.083098
103.100699	2840.736165	23.088115
102.967762	2851.956693	23.093133
103.301166	2865.613203	23.098151
103.480992	2870.523612	23.103168
103.418388	2872.298720	23.108186
103.795069	2877.955339	23.113203
103.740234	2879.918940	23.118221
103.896359	2873.058354	23.123239
103.882026	2868.352926	23.128256
103.909751	2887.475834	23.133274
104.316355	2893.724796	23.138291
104.083810	2900.698132	23.143309
104.363972	2904.766285	23.148327
104.389892	2901.905116	23.153344
103.979096	2905.937261	23.158362
104.357383	2920.166355	23.163379
104.847607	2934.156439	23.168397
104.781627	2934.826118	23.173415
105.063780	2931.732349	23.178432
104.787058	2943.125185	23.183450
105.263497	2952.010067	23.188467
105.306607	2953.722796	23.193485
105.802902	2961.388549	23.198503
105.797286	2955.915447	23.203520
105.869777	2949.312001	23.208538
105.999050	2948.374029	23.213555
105.854266	2956.331366	23.218573
106.051124	2946.124754	23.223591
105.950356	2938.104606	23.228608
106.020762	2948.854100	23.233626
106.512742	2954.927521	23.238643
106.540806	2969.071325	23.243661
106.458162	2970.110330	23.248679
106.599286	2972.108040	23.253696
106.577293	2972.310951	23.258714
106.870989	2957.473743	23.263731
106.624505	2974.557733	23.268749
106.795931	2987.098947	23.273767
107.339196	2994.253354	23.278784
107.342819	2995.991525	23.283802
107.149232	2991.932719	23.288819
107.391115	2992.769559	23.293837
107.262881	3000.846236	23.298855
107.353451	3015.970370	23.303872
107.038488	3026.611658	23.308890
107.562659	3027.931336	23.313907
107.407038	3046.087069	23.318925
107.696945	3054.216998	23.323943
107.758191	3054.605752	23.328960
107.994930	3072.326838	23.333978
108.236320	3073.114940	23.338995
108.393823	3080.119063	23.344013
108.575277	3083.688204	23.349031
109.113430	3074.835761	23.354048
108.835612	3070.336902	23.359066
109.101985	3073.142309	23.364083
108.848823	3073.705964	23.369101
109.424793	3094.311332	23.374119
109.797214	3093.685883	23.379136
109.201128	3109.242324	23.384154
109.344217	3096.464358	23.389171
109.876300	3101.596467	23.394189
109.511278	3099.884732	23.399207
109.667060	3088.768603	23.404224
109.825186	3099.774963	23.409242
110.146807	3104.195392	23.414259
110.441583	3123.774422	23.419277
110.299528	3127.271926	23.424295
110.444429	3121.318292	23.429312
110.472285	3123.180823	23.434330
110.639314	3121.337687	23.439347
110.677932	3114.867351	23.444365
110.779536	3123.801791	23.449383
110.720889	3119.735179	23.454400
110.515451	3142.877293	23.459418
110.798792	3149.163303	23.464435
110.901656	3148.692333	23.469453
111.101448	3171.527612	23.474471
111.340008	3179.958262	23.479488
111.493304	3191.747451	23.484506
111.450874	3178.898155	23.489523
111.633479	3187.586128	23.494541
111.563600	3201.812900	23.499559
112.336177	3208.740053	23.504576
111.953984	3215.176045	23.509594
112.316023	3203.016532	23.514611
112.398661	3214.374873	23.519629
112.173222	3211.681260	23.524647
112.574156	3215.069593	23.529664
112.582040	3228.852764	23.534682
112.782637	3230.056331	23.539699
113.050885	3224.289737	23.544717
113.067645	3221.593035	23.549735
113.286100	3228.594221	23.554752
113.211820	3251.722261	23.559770
113.498390	3260.458817	23.564787
113.626587	3260.680965	23.569805
113.463476	3246.638478	23.574823
113.735044	3250.833748	23.579840
113.667171	3258.511549	23.584858
113.954857	3261.731221	23.589875
114.211089	3277.203022	23.594893
114.080738	3278.272782	23.599911
114.061965	3283.483946	23.604928
114.303675	3290.497453	23.609946
114.454097	3283.521085	23.614963
114.705160	3289.920775	23.619981
114.740446	3307.956219	23.624999
115.046626	3304.209513	23.630016
114.923266	3304.893432	23.635034
115.064481	3304.689759	23.640051
114.992356	3303.021644	23.645069
114.929418	3320.287062	23.650087
115.554102	3329.952034	23.655104
115.640468	3329.764136	23.660122
115.494290	3332.007116	23.665139
115.991956	3343.065319	23.670157
115.818367	3338.195151	23.675175
116.023055	3345.647142	23.680192
116.096960	3368.327154	23.685210
116.112959	3368.060343	23.690227
116.241355	3360.965921	23.695245
116.676053	3366.480029	23.700263
117.267868	3358.813554	23.705280
116.483360	3363.814083	23.710298
116.569671	3361.316494	23.715315
117.125404	3348.990534	23.720333
116.767823	3362.935129	23.725351
117.399624	3364.858346	23.730368
117.394312	3371.683234	23.735386
117.194228	3378.726613	23.740403
117.546143	3373.950553	23.745421
117.188706	3380.656952	23.750439
117.305281	3384.617655	23.755456
117.618016	3392.794381	23.760474
117.616815	3405.830311	23.765491
118.324426	3402.940452	23.770509
117.889928	3413.169460	23.775527
118.361182	3420.238733	23.780544
118.216987	3437.972903	23.785562
118.404508	3444.167404	23.790579
118.789078	3432.500891	23.795597
118.626324	3436.887817	23.800615
118.994361	3444.849092	23.805632
119.047940	3458.775705	23.810650
119.149229	3463.410295	23.815667
119.749272	3460.994586	23.820685
119.323048	3461.392789	23.825703
119.584889	3460.882496	23.830720
119.589138	3459.759658	23.835738
119.530919	3465.884210	23.840755
119.762375	3482.386812	23.845773
119.759173	3492.872458	23.850791
120.018378	3488.063676	23.855808
120.022104	3495.547434	23.860826
120.540657	3518.839168	23.865843
120.630143	3517.436041	23.870861
120.528967	3522.141181	23.875879
120.771937	3522.476236	23.880896
120.593300	3524.610038	23.885914
120.861821	3528.177074	23.890931
121.007202	3533.311925	23.895949
121.133996	3549.703958	23.900967
121.267439	3548.047064	23.905984
121.418465	3548.457586	23.911002
121.278571	3552.655304	23.916019
121.690278	3567.505125	23.921037
121.981147	3583.625511	23.926055
122.234727	3581.444332	23.931072
122.280787	3584.914730	23.936090
122.448189	3581.088954	23.941107
122.587012	3583.882103	23.946125
122.067704	3586.389282	23.951143
122.420868	3578.300345	23.956160
122.149182	3595.258459	23.961178
122.528679	3606.282075	23.966195
122.847157	3597.958684	23.971213
122.436234	3620.136580	23.976231
123.064191	3624.089461	23.981248
123.180847	3631.123432	23.986266
123.051121	3640.007478	23.991283
122.958307	3640.175267	23.996301
123.708064	3654.643965	24.001319
123.804789	3654.555148	24.006336
123.759750	3657.935514	24.011354
123.917827	3663.773908	24.016371
123.899488	3684.434745	24.021389
123.859551	3686.143978	24.026407
124.331913	3685.181844	24.031424
124.541776	3687.838824	24.036442
124.662977	3684.638862	24.041459
125.052322	3677.879883	24.046477
124.966042	3698.130279	24.051495
125.222935	3702.578922	24.056512
125.301692	3699.891561	24.061530
125.362975	3711.398307	24.066547
125.617230	3698.792416	24.071565
125.700536	3704.363641	24.076583
125.550365	3704.189305	24.081600
125.654130	3702.369176	24.086618
125.916361	3709.736214	24.091635
125.865783	3697.741889	24.096653
125.730738	3735.895647	24.101671
126.170894	3731.103691	24.106688
126.230912	3737.031979	24.111706
126.081026	3733.554798	24.116723
126.455443	3748.781879	24.121741
126.464346	3765.806730	24.126759
126.937073	3754.731764	24.131776
127.065068	3758.466232	24.136794
127.212535	3763.639403	24.141811
127.410555	3784.883533	24.146829
127.583653	3794.287294	24.151847
127.726091	3789.855282	24.156864
127.701886	3794.840713	24.161882
127.560514	3794.091613	24.166899
128.136524	3778.850544	24.171917
127.744983	3791.421820	24.176935
128.067607	3799.796756	24.181952
128.236444	3803.535499	24.186970
128.102912	3810.525920	24.191987
128.234695	3804.054837	24.197005
128.518301	3824.658783	24.202023
128.616568	3831.330877	24.207040
128.383727	3835.830712	24.212058
128.658264	3843.539131	24.217075
129.045516	3850.652434	24.222093
128.981735	3860.256104	24.227111
129.017131	3871.912549	24.232128
129.550795	3882.240666	24.237146
129.578455	3897.641853	24.242163
129.979884	3889.976718	24.247181
129.857084	3895.378561	24.252199
130.137909	3901.378638	24.257216
130.222377	3906.470146	24.262234
130.337167	3916.179740	24.267251
130.385483	3914.959403	24.272269
130.517057	3921.728004	24.277287
130.339787	3916.351893	24.282304
130.820255	3934.236392	24.287322
130.604507	3946.328622	24.292339
131.555116	3934.855863	24.297357
131.305232	3947.627072	24.302375
131.470055	3952.986435	24.307392
131.606166	3971.863557	24.312410
131.803731	3974.825818	24.317427
132.030216	3968.741017	24.322445
131.858644	3981.205150	24.327463
131.646532	3978.535184	24.332480
131.936625	3984.375468	24.337498
131.946171	3999.151708	24.342515
132.256331	4008.241918	24.347533
131.902203	4008.612445	24.352551
132.531336	4017.536450	24.357568
133.025642	4029.457245	24.362586
132.810312	4030.864007	24.367603
133.192633	4024.407664	24.372621
133.138556	4033.024252	24.377639
133.233858	4045.945904	24.382656
133.708937	4049.679682	24.387674
133.663600	4058.131032	24.392691
133.866028	4049.103278	24.397709
133.723216	4054.356103	24.402727
133.852102	4054.196202	24.407744
134.264217	4068.316794	24.412762
134.143450	4083.872284	24.417779
134.391916	4077.504232	24.422797
134.389908	4083.788249	24.427815
134.711595	4084.671397	24.432832
134.817160	4080.450951	24.437850
134.791561	4101.583691	24.442867
134.977551	4107.734215	24.447885
135.049830	4104.023289	24.452903
134.929432	4114.551984	24.457920
135.592284	4114.034348	24.462938
135.540855	4135.863644	24.467955
135.667629	4132.046824	24.472973
135.948300	4131.756265	24.477991
135.874364	4129.786345	24.483008
136.069952	4143.089962	24.488026
136.367178	4161.101923	24.493043
137.066073	4154.312757	24.498061
137.221983	4158.351410	24.503079
137.067594	4157.055541	24.508096
136.942068	4147.597696	24.513114
137.119249	4153.860738	24.518131
137.142237	4153.056058	24.523149
137.015660	4157.951056	24.528167
137.455013	4176.114336	24.533184
137.471448	4181.729090	24.538202
137.374001	4183.799924	24.543219
137.924993	4189.448249	24.548237
137.851411	4201.615973	24.553255
137.897292	4215.890259	24.558272
138.012928	4211.407439	24.563290
138.170462	4223.833029	24.568307
138.188560	4233.148918	24.573325
138.572323	4236.649787	24.578343
138.335395	4235.199044	24.583360
138.788239	4249.354796	24.588378
139.077753	4271.723210	24.593395
139.299103	4271.519648	24.598413
139.290515	4283.306535	24.603431
139.140849	4275.809629	24.608448
139.689771	4283.646885	24.613466
139.512628	4298.319645	24.618483
139.686322	4306.839610	24.623501
140.069571	4306.339908	24.628519
139.904444	4312.058008	24.633536
140.383634	4327.774300	24.638554
140.026174	4333.167496	24.643571
140.633369	4337.095256	24.648589
140.627439	4351.396356	24.653607
140.639279	4352.170160	24.658624
141.065480	4353.428214	24.663642
140.847825	4365.200160	24.668659
141.325895	4370.017172	24.673677
141.316599	4379.847220	24.678695
141.444651	4380.481292	24.683712
142.150433	4381.313470	24.688730
141.755345	4383.257984	24.693747
141.967883	4389.234116	24.698765
142.494895	4394.869949	24.703783
142.331184	4404.820080	24.708800
142.603505	4393.112376	24.713818
142.780013	4391.312809	24.718835
142.608682	4392.230345	24.723853
142.676276	4401.045927	24.728871
142.982347	4416.999668	24.733888
143.380777	4415.522476	24.738906
143.418333	4426.941926	24.743923
143.366266	4420.384078	24.748941
143.560201	4429.665460	24.753959
143.323908	4433.302891	24.758976
143.472996	4439.073761	24.763994
143.677914	4450.695483	24.769011
143.979655	4452.797132	24.774029
143.975875	4467.029465	24.779047
143.815086	4479.568598	24.784064
144.391575	4481.391653	24.789082
144.211450	4493.399257	24.794099
144.484434	4509.402671	24.799117
145.028623	4504.818105	24.804135
145.037046	4513.960140	24.809152
145.564332	4521.429377	24.814170
145.360143	4533.207882	24.819187
145.841554	4539.363221	24.824205
145.825752	4539.109925	24.829223
146.004122	4537.525033	24.834240
146.160665	4526.739713	24.839258
145.970142	4540.301325	24.844275
146.563286	4550.877568	24.849293
146.380838	4558.105988	24.854311
146.404282	4568.894690	24.859328
146.887930	4561.455822	24.864346
146.772081	4570.663353	24.869363
147.024635	4590.511101	24.874381
147.012015	4585.437483	24.879399
147.258554	4587.760928	24.884416
147.668413	4609.497975	24.889434
147.640688	4615.665967	24.894451
147.746723	4619.519260	24.899469
147.757834	4611.189125	24.904487
147.566130	4630.685195	24.909504
148.110047	4647.106189	24.914522
148.540086	4645.129949	24.919539
148.610654	4652.951291	24.924557
148.442990	4658.195043	24.929575
148.786571	4663.113955	24.934592
149.100945	4672.567704	24.939610
149.027638	4666.925256	24.944627
149.183879	4673.031312	24.949645
149.624347	4687.958949	24.954663
149.773486	4697.488897	24.959680
149.979116	4695.284398	24.964698
149.755560	4699.389163	24.969715
149.956540	4696.891675	24.974733
150.196549	4702.415261	24.979751
150.036591	4717.516359	24.984768
150.540179	4719.920127	24.989786
150.493397	4724.652454	24.994803
150.534875	4740.979527	24.999821
151.121691	4744.418544	25.004839
150.851565	4757.988009	25.009856
151.144758	4751.365777	25.014874
151.415521	4761.022902	25.019891
151.569001	4778.972740	25.024909
151.726410	4775.017596	25.029927
151.709147	4781.763563	25.034944
152.224987	4779.010747	25.039962
152.250988	4781.461301	25.044979
152.073222	4803.760559	25.049997
152.599253	4804.869816	25.055015
152.317206	4813.207186	25.060032
152.888975	4812.177736	25.065050
152.845768	4801.443411	25.070067
152.849722	4813.848428	25.075085
153.222563	4820.071470	25.080103
153.197694	4837.542925	25.085120
153.337394	4833.145727	25.090138
153.286667	4842.100067	25.095155
153.362913	4865.409542	25.100173
153.722897	4861.761854	25.105191
153.914549	4857.612006	25.110208
154.120707	4878.383734	25.115226
154.124197	4885.588609	25.120243
154.278762	4895.996699	25.125261
154.411565	4899.657402	25.130279
154.393023	4915.200727	25.135296
154.992771	4916.773478	25.140314
155.010069	4922.041826	25.145331
155.213394	4936.738038	25.150349
155.681864	4943.081546	25.155367
155.677755	4947.285507	25.160384
155.803144	4943.995602	25.165402
155.737023	4951.547535	25.170419
156.004230	4968.039090	25.175437
156.198048	4976.085122	25.180455
155.704402	4977.837317	25.185472
156.453323	4995.074524	25.190490
156.752351	4992.548157	25.195507
156.694459	4997.521038	25.200525
156.854156	5002.071990	25.205543
157.184568	5030.958150	25.210560
157.376543	5033.345038	25.215578
157.187259	5031.609894	25.220595
157.288666	5047.747797	25.225613
157.475592	5052.041445	25.230631
157.912927	5071.910404	25.235648
158.027792	5087.597991	25.240666
158.235291	5087.999996	25.245683
158.258592	5106.348219	25.250701
158.568760	5101.941627	25.255719
158.737980	5115.994692	25.260736
158.895666	5119.607222	25.265754
159.284728	5110.525913	25.270771
159.154974	5118.296379	25.275789
159.623466	5134.194821	25.280807
159.459746	5142.220584	25.285824
159.610587	5145.516860	25.290842
159.777389	5145.846846	25.295859
159.818515	5158.243618	25.300877
160.258765	5168.919625	25.305895
160.394109	5172.565794	25.310912
160.440068	5171.260298	25.315930
160.737772	5172.185287	25.320947
160.661472	5194.520280	25.325965
160.866685	5194.082319	25.330983
161.081745	5207.122139	25.336000
160.936989	5215.604746	25.341018
161.464352	5222.715960	25.346035
161.202696	5237.624894	25.351053
161.946358	5241.493281	25.356071
161.977843	5257.172001	25.361088
162.232773	5254.952963	25.366106
162.498361	5261.311286	25.371123
162.603872	5275.065521	25.376141
162.773829	5276.202259	25.381159
162.984593	5281.716716	25.386176
163.092528	5280.950684	25.391194
163.086906	5280.268033	25.396211
163.344661	5281.746225	25.401229
163.355224	5282.862884	25.406247
163.357297	5303.223975	25.411264
163.521911	5303.046335	25.416282
163.624768	5316.993216	25.421299
163.635630	5338.236566	25.426317
164.173900	5337.448908	25.431335
164.414984	5346.002386	25.436352
164.129648	5355.944110	25.441370
164.315542	5362.131373	25.446387
164.577123	5384.776926	25.451405
165.035909	5387.646594	25.456423
164.675653	5401.982103	25.461440
165.044518	5406.293772	25.466458
165.784001	5418.273490	25.471475
165.422998	5435.492518	25.476493
165.779037	5434.672805	25.481511
165.753841	5442.108721	25.486528
166.155666	5453.757658	25.491546
166.534265	5463.745479	25.496563
166.575448	5462.977100	25.501581
166.727257	5461.626492	25.506599
166.900628	5484.878274	25.511616
166.977148	5489.597506	25.516634
166.697602	5492.353933	25.521651
166.922836	5507.061228	25.526669
167.705917	5515.374641	25.531687
167.784151	5519.412329	25.536704
167.738846	5521.421147	25.541722
167.883393	5526.289010	25.546739
168.243678	5545.206519	25.551757
168.504804	5550.682017	25.556775
168.727160	5552.523664	25.561792
168.650274	5568.082804	25.566810
168.784086	5562.894056	25.571827
168.806860	5568.961124	25.576845
168.886340	5580.843090	25.581863
169.337315	5594.450627	25.586880
169.392178	5595.929358	25.591898
169.708508	5603.596285	25.596915
169.821944	5617.794500	25.601933
169.987603	5624.657826	25.606951
169.921672	5631.754819	25.611968
170.314555	5654.573561	25.616986
170.530358	5657.573292	25.622003
170.557387	5669.318302	25.627021
171.121693	5678.733647	25.632039
170.711358	5689.635882	25.637056
171.190273	5691.868255	25.642074
171.557501	5703.626281	25.647091
171.595828	5710.858057	25.652109
171.960202	5716.412608	25.657127
172.008142	5716.737869	25.662144
172.188896	5728.173936	25.667162
172.566224	5733.567253	25.672180
172.793685	5740.603910	25.677197
172.916554	5734.609622	25.682215
172.737810	5740.810143	25.687232
172.880556	5755.114681	25.692250
173.385654	5766.821577	25.697268
173.056730	5771.309510	25.702285
173.472747	5778.073174	25.707303
173.787717	5801.851732	25.712320
173.769255	5797.968768	25.717338
174.058866	5792.207553	25.722356
174.077216	5806.414590	25.727373
174.341242	5816.924098	25.732391
174.286713	5824.292590	25.737408
174.381173	5828.477317	25.742426
175.013395	5838.870753	25.747444
175.128364	5858.249834	25.752461
175.447468	5854.711080	25.757479
175.647795	5857.716562	25.762496
175.548522	5856.776876	25.767514
175.796644	5855.170857	25.772532
175.605534	5877.709334	25.777549
175.979734	5878.281455	25.782567
176.232004	5880.124490	25.787584
176.408797	5899.643034	25.792602
176.675526	5903.510208	25.797620
176.306682	5915.345352	25.802637
176.577509	5920.022307	25.807655
176.841155	5933.984859	25.812672
176.718571	5941.560788	25.817690
177.148315	5954.503466	25.822708
177.103352	5973.062476	25.827725
177.554874	5981.089202	25.832743
177.987841	6003.509579	25.837760
178.050695	6001.661700	25.842778
178.519933	6007.737726	25.847796
178.431584	6014.495200	25.852813
178.790809	6018.781069	25.857831
178.906774	6032.985539	25.862848
178.923691	6059.895786	25.867866
179.621499	6039.706997	25.872884
179.554935	6054.458382	25.877901
179.728915	6067.555336	25.882919
180.049405	6073.736350	25.887936
180.098297	6085.703310	25.892954
180.429140	6077.954295	25.897972
180.288149	6092.834606	25.902989
180.592639	6096.933439	25.908007
180.783625	6104.369322	25.913024
180.700658	6108.075478	25.918042
181.397961	6115.465354	25.923060
181.617664	6130.288352	25.928077
181.493931	6132.738699	25.933095
181.608096	6137.547983	25.938112
181.615818	6139.939552	25.943130
182.179110	6164.190292	25.948148
182.282459	6158.585012	25.953165
182.248287	6171.164384	25.958183
182.419053	6174.775780	25.963200
182.650978	6196.290075	25.968218
183.042511	6192.324176	25.973236
183.279904	6204.437237	25.978253
183.316411	6225.759448	25.983271
183.325300	6217.288636	25.988288
183.414430	6237.216710	25.993306
183.967727	6245.030604	25.998324
183.844774	6256.188102	26.003341
184.235224	6259.610350	26.008359
184.633598	6279.586526	26.013376
184.744277	6277.395954	26.018394
184.952936	6276.410780	26.023412
184.465706	6292.882903	26.028429
184.853737	6303.640791	26.033447
184.987395	6308.117669	26.038464
184.972962	6333.229101	26.043482
185.825349	6341.329062	26.048500
186.186838	6340.932153	26.053517
185.575148	6362.650127	26.058535
186.251302	6365.739190	26.063552
186.453515	6367.979663	26.068570
186.551166	6375.798952	26.073588
186.774515	6396.435147	26.078605
187.064622	6393.146818	26.083623
187.493019	6395.886234	26.088640
187.055060	6396.250989	26.093658
187.495298	6415.193327	26.098676
187.724303	6422.474990	26.103693
187.898657	6424.170310	26.108711
187.856274	6418.393730	26.113728
187.854813	6436.453806	26.118746
188.510412	6441.980884	26.123764
188.624504	6451.854806	26.128781
188.218667	6466.250015	26.133799
188.730359	6470.591896	26.138816
189.328770	6493.685009	26.143834
189.698772	6503.058190	26.148852
190.132835	6497.861179	26.153869
190.033856	6496.301530	26.158887
190.158812	6498.014488	26.163904
190.228737	6513.540013	26.168922
190.544300	6518.442885	26.173940
190.260389	6525.358972	26.178957
190.441324	6542.137407	26.183975
190.942217	6546.417298	26.188992
190.453764	6562.482689	26.194010
191.016496	6577.257984	26.199028
191.459938	6581.629311	26.204045
191.342272	6584.290600	26.209063
191.587689	6602.933026	26.214080
192.031431	6618.500741	26.219098
191.941565	6630.257151	26.224116
191.956891	6638.679360	26.229133
192.281773	6654.677153	26.234151
192.784508	6681.385158	26.239168
192.569702	6688.740413	26.244186
193.169975	6697.068183	26.249204
193.428236	6718.752900	26.254221
193.246702	6721.329478	26.259239
193.842918	6732.774687	26.264256
193.997939	6752.602710	26.269274
194.177889	6748.540163	26.274292
194.550449	6769.532582	26.279309
194.624336	6774.751221	26.284327
194.918461	6766.672409	26.289344
194.800257	6791.207063	26.294362
195.239012	6798.545546	26.299380
195.443921	6808.527531	26.304397
195.427418	6812.521371	26.309415
196.141431	6821.494375	26.314432
195.935573	6826.615198	26.319450
196.284499	6827.256919	26.324468
196.231476	6843.820777	26.329485
196.729290	6849.441859	26.334503
196.796950	6854.682822	26.339520
196.841824	6867.641915	26.344538
197.426731	6883.476383	26.349556
197.550651	6888.522943	26.354573
197.451175	6896.645290	26.359591
198.029614	6911.434052	26.364608
198.137212	6920.787120	26.369626
198.357473	6918.363288	26.374644
198.365334	6930.278604	26.379661
198.695121	6936.788450	26.384679
198.985989	6938.123480	26.389696
198.799606	6949.154911	26.394714
198.818027	6954.484400	26.399732
199.364868	6974.232871	26.404749
199.157968	6979.012069	26.409767
199.445588	6984.471866	26.414784
199.521224	7008.743980	26.419802
199.708871	7010.422987	26.424820
200.043924	7030.977716	26.429837
200.092398	7036.568490	26.434855
200.626434	7050.833844	26.439872
200.446243	7063.330183	26.444890
200.561007	7071.720407	26.449908
200.965649	7088.644340	26.454925
201.078706	7097.548424	26.459943
201.653903	7102.907095	26.464960
201.840567	7113.097875	26.469978
201.854550	7125.473113	26.474996
202.290407	7141.699570	26.480013
202.474024	7148.849663	26.485031
202.931928	7142.685171	26.490048
202.914331	7152.325335	26.495066
203.121484	7167.697242	26.500084
203.298504	7172.716986	26.505101
203.481918	7183.846473	26.510119
203.771213	7189.812541	26.515136
203.950295	7210.857266	26.520154
203.837794	7213.019991	26.525172
204.335191	7227.126157	26.530189
204.306807	7250.715613	26.535207
204.608707	7249.552684	26.540224
204.832905	7258.888225	26.545242
205.288609	7268.673023	26.550260
205.268403	7276.999842	26.555277
205.558409	7295.775122	26.560295
205.576949	7289.596661	26.565312
205.422098	7311.722360	26.570330
205.780666	7317.251660	26.575348
206.538700	7339.859579	26.580365
206.381981	7351.890676	26.585383
206.764248	7362.525786	26.590400
206.832059	7388.606727	26.595418
207.427852	7394.704880	26.600436
207.671179	7400.276917	26.605453
207.826984	7409.682945	26.610471
208.308820	7405.737248	26.615488
208.318071	7407.090581	26.620506
208.270881	7412.099468	26.625524
208.712198	7420.557911	26.630541
208.745395	7431.747097	26.635559
208.978422	7434.576541	26.640576
209.079613	7444.712367	26.645594
209.411268	7465.818031	26.650612
209.769348	7463.324830	26.655629
209.596571	7477.658737	26.660647
210.333475	7491.138661	26.665664
210.425395	7499.364327	26.670682
210.599347	7496.438437	26.675700
210.871898	7506.727893	26.680717
210.928042	7516.979137	26.685735
211.149842	7514.324167	26.690752
211.048837	7527.624599	26.695770
211.114192	7547.856791	26.700788
212.086419	7550.758451	26.705805
211.336477	7565.900845	26.710823
212.072079	7579.928510	26.715840
211.774996	7582.493633	26.720858
212.029450	7606.801649	26.725876
212.461263	7629.515973	26.730893
212.522485	7649.468557	26.735911
212.721201	7650.514852	26.740928
212.964603	7671.143872	26.745946
213.353941	7679.866275	26.750964
213.550126	7690.174793	26.755981
213.648097	7708.544387	26.760999
213.838150	7715.857514	26.766016
214.206745	7726.807852	26.771034
214.273505	7746.029438	26.776052
214.505696	7742.000529	26.781069
214.584724	7764.815192	26.786087
215.018444	7770.448792	26.791104
215.566636	7799.245668	26.796122
215.496573	7807.948876	26.801140
215.940077	7797.165036	26.806157
215.673903	7817.677735	26.811175
216.082310	7826.081978	26.816192
216.696578	7842.218178	26.821210
216.840607	7851.926535	26.826228
217.101186	7855.317070	26.831245
217.223343	7868.163358	26.836263
217.233474	7873.769438	26.841280
217.605211	7880.928108	26.846298
217.850296	7882.423616	26.851316
218.260265	7891.341223	26.856333
218.370944	7903.069313	26.861351
218.355581	7907.885611	26.866368
218.963845	7929.302148	26.871386
218.742180	7947.637493	26.876404
219.053658	7943.172406	26.881421
218.977493	7964.949631	26.886439
219.295994	7968.995435	26.891456
219.409964	7989.142156	26.896474
219.874449	8011.056809	26.901492
219.927978	8021.126059	26.906509
220.186920	8037.058967	26.911527
220.458489	8054.924441	26.916544
220.703422	8070.539887	26.921562
221.068170	8083.194161	26.926580
221.200042	8094.730617	26.931597
221.324483	8103.483712	26.936615
221.461055	8125.292897	26.941632
221.909222	8127.737103	26.946650
221.876051	8153.630416	26.951668
222.484591	8164.754811	26.956685
222.526416	8177.716263	26.961703
222.632180	8191.629744	26.966720
222.845024	8199.534842	26.971738
222.859029	8226.401972	26.976756
223.929243	8224.413867	26.981773
223.878425	8249.116846	26.986791
224.015729	8252.586953	26.991808
224.540677	8255.524981	26.996826
224.536517	8278.316338	27.001844
224.864093	8287.618042	27.006861
224.759982	8292.687829	27.011879
224.884979	8309.538046	27.016896
225.327051	8312.771811	27.021914
225.527881	8335.693954	27.026932
225.979853	8344.518213	27.031949
225.652724	8349.799025	27.036967
226.365017	8359.502639	27.041984
226.757876	8372.354938	27.047002
226.869873	8372.996562	27.052020
227.244084	8387.453428	27.057037
227.209768	8403.908676	27.062055
227.061424	8406.572194	27.067072
227.649053	8429.780199	27.072090
227.455896	8440.334045	27.077108
228.217800	8453.081994	27.082125
228.155927	8467.084120	27.087143
228.384685	8478.818295	27.092160
228.583200	8486.103593	27.097178
228.869770	8504.242797	27.102196
229.321353	8512.871855	27.107213
229.447409	8528.923357	27.112231
229.500575	8529.333676	27.117248
229.773109	8545.123836	27.122266
230.045240	8566.152585	27.127284
229.965129	8571.079844	27.132301
230.177580	8590.288570	27.137319
230.243889	8600.950031	27.142336
230.859047	8614.702360	27.147354
230.897386	8635.822680	27.152372
231.092694	8645.099223	27.157389
231.165731	8660.089081	27.162407
231.336774	8683.627948	27.167424
231.449020	8697.143769	27.172442
231.965023	8726.599122	27.177460
232.399631	8729.040942	27.182477
232.544289	8741.647094	27.187495
233.049731	8764.446168	27.192512
233.138694	8783.715744	27.197530
233.523528	8789.758769	27.202548
233.738053	8808.865795	27.207565
233.779413	8815.994498	27.212583
234.166812	8828.686579	27.217600
234.786549	8846.535483	27.222618
234.572720	8849.298142	27.227636
235.167916	8865.869446	27.232653
235.334648	8871.527942	27.237671
235.416418	8884.622000	27.242688
235.742676	8890.367534	27.247706
235.909533	8906.211781	27.252724
236.333489	8914.914954	27.257741
236.255419	8933.821629	27.262759
236.500286	8944.308025	27.267776
237.003045	8959.698902	27.272794
237.316859	8967.386001	27.277812
237.410368	8975.943027	27.282829
237.253337	8983.455200	27.287847
237.547803	9006.892184	27.292864
238.006318	9016.227784	27.297882
238.256216	9038.087203	27.302900
238.835069	9049.753605	27.307917
238.859506	9062.097102	27.312935
238.806028	9078.216685	27.317952
239.409363	9081.362471	27.322970
239.502270	9097.854880	27.327988
239.276066	9108.665146	27.333005
239.693503	9121.032652	27.338023
240.324445	9138.216724	27.343040
240.665916	9153.965352	27.348058
240.613650	9167.130670	27.353076
241.229567	9168.460145	27.358093
241.437377	9189.776871	27.363111
241.542902	9209.497189	27.368128
241.858303	9204.419003	27.373146
241.942166	9220.890978	27.378164
242.422952	9238.158309	27.383181
242.760850	9233.471068	27.388199
242.647435	9243.842081	27.393216
243.048766	9261.473151	27.398234
243.250999	9271.450823	27.403252
243.422491	9285.711241	27.408269
243.853982	9294.837989	27.413287
243.839892	9304.107825	27.418304
244.310547	9324.283053	27.423322
244.220875	9336.823689	27.428340
244.663867	9344.647144	27.433357
244.939413	9348.412084	27.438375
244.732737	9366.651246	27.443392
245.136571	9365.654854	27.448410
245.235582	9388.227464	27.453428
245.070063	9395.501747	27.458445
245.367670	9418.830888	27.463463
245.174185	9433.683608	27.468480
245.682670	9456.240527	27.473498
246.363759	9487.019437	27.478516
246.614164	9506.215891	27.483533
247.143977	9518.012862	27.488551
247.269200	9539.816400	27.493568
247.997729	9545.971411	27.498586
247.800930	9560.253646	27.503604
248.308852	9572.983091	27.508621
248.788465	9579.765438	27.513639
248.656749	9603.174578	27.518656
249.037272	9605.749174	27.523674
249.295645	9615.752432	27.528692
249.547049	9640.464249	27.533709
249.665243	9638.125447	27.538727
250.084397	9653.998786	27.543744
250.342478	9661.254278	27.548762
250.417794	9674.561180	27.553780
250.546007	9688.646350	27.558797
250.623648	9695.240036	27.563815
250.976340	9723.390511	27.568832
251.342717	9727.613976	27.573850
251.794003	9757.217442	27.578868
251.900392	9762.871274	27.583885
252.084450	9778.856917	27.588903
252.131041	9798.178055	27.593920
252.633566	9810.486319	27.598938
252.733808	9832.636297	27.603956
253.396772	9843.836370	27.608973
253.667139	9850.681042	27.613991
253.950434	9871.618273	27.619008
254.204155	9876.869610	27.624026
254.172975	9892.558538	27.629044
254.457782	9898.915549	27.634061
254.978080	9924.528668	27.639079
254.967619	9942.823450	27.644096
255.305962	9949.952343	27.649114
255.462755	9969.104184	27.654132
255.711844	9979.462935	27.659149
256.260570	9995.050458	27.664167
255.995515	10014.731478	27.669184
256.713313	10032.096727	27.674202
256.920462	10043.272338	27.679220
257.387347	10067.461485	27.684237
257.753589	10069.677701	27.689255
257.500220	10079.628875	27.694272
257.929478	10094.588683	27.699290
257.971418	10100.529827	27.704308
258.212988	10122.127395	27.709325
259.014804	10125.219269	27.714343
258.706160	10158.421983	27.719360
259.341552	10160.035881	27.724378
259.221732	10182.808120	27.729396
259.753892	10188.077284	27.734413
259.824556	10203.173757	27.739431
259.916440	10221.714261	27.744448
260.621220	10235.524061	27.749466
261.035456	10258.093772	27.754484
261.021942	10259.624437	27.759501
261.271660	10286.441817	27.764519
261.584801	10294.103669	27.769536
261.961023	10307.229720	27.774554
262.463225	10317.040217	27.779572
262.349275	10322.135905	27.784589
262.701121	10323.992925	27.789607
262.495968	10337.658782	27.794624
262.998313	10342.944751	27.799642
263.056000	10357.751231	27.804660
263.281102	10374.461782	27.809677
263.644163	10393.487809	27.814695
263.648373	10404.240319	27.819712
264.146163	10424.254087	27.824730
264.569212	10442.424106	27.829748
264.445019	10456.652572	27.834765
264.622265	10472.604580	27.839783
264.742422	10499.073476	27.844800
265.385844	10516.650099	27.849818
265.819718	10524.488250	27.854836
266.131453	10550.894795	27.859853
266.932752	10564.087780	27.864871
266.648671	10571.545300	27.869888
266.833848	10586.660206	27.874906
267.395077	10598.366114	27.879924
267.501240	10628.482111	27.884941
267.891192	10632.640463	27.889959
267.705119	10658.572576	27.894976
268.307114	10665.823596	27.899994
268.857250	10686.522333	27.905012
268.952780	10697.632575	27.910029
269.443741	10713.331992	27.915047
269.511725	10733.612676	27.920064
269.545258	10731.224703	27.925082
269.967548	10759.665644	27.930100
270.144377	10771.789840	27.935117
270.568735	10788.477294	27.940135
270.663881	10808.312378	27.945152
271.297137	10819.776472	27.950170
271.279347	10830.818898	27.955188
271.483966	10851.921697	27.960205
272.002088	10855.693327	27.965223
272.177005	10875.827281	27.970240
272.579270	10889.760992	27.975258
272.448137	10907.312618	27.980276
273.130848	10923.034076	27.985293
273.866399	10932.133494	27.990311
273.808258	10953.388643	27.995328
274.100279	10955.891446	28.000346
274.224852	10975.680895	28.005364
274.143278	10992.373518	28.010381
275.076016	11004.265620	28.015399
274.727388	11013.240424	28.020416
275.175028	11030.430085	28.025434
275.567461	11043.149091	28.030452
275.767819	11064.331659	28.035469
276.353397	11073.832583	28.040487
276.784347	11092.211602	28.045504
276.727506	11098.884850	28.050522
276.978716	11101.608732	28.055540
277.265992	11126.954282	28.060557
277.476217	11129.677074	28.065575
277.619529	11155.082739	28.070592
277.868033	11163.824849	28.075610
278.393435	11187.886240	28.080628
278.294310	11195.088100	28.085645
279.009885	11209.743921	28.090663
278.960968	11243.841867	28.095680
279.578978	11241.577680	28.100698
279.758998	11261.016363	28.105716
279.785538	11273.058661	28.110733
280.330445	11289.766076	28.115751
280.404630	11296.349960	28.120768
280.614536	11317.123159	28.125786
281.170470	11317.128878	28.130804
281.277320	11337.917585	28.135821
281.476379	11338.409406	28.140839
281.508426	11362.064232	28.145856
281.879981	11376.584905	28.150874
282.235634	11393.330056	28.155892
282.244409	11402.116703	28.160909
282.239134	11423.251839	28.165927
282.209927	11453.188505	28.170944
282.564173	11472.704181	28.175962
283.310619	11502.397519	28.180980
283.088276	11528.822368	28.185997
284.043103	11552.663526	28.191015
284.456795	11570.560606	28.196032
284.802089	11593.591911	28.201050
285.362284	11609.512385	28.206068
285.525645	11636.640976	28.211085
285.939620	11631.764757	28.216103
286.164195	11657.624194	28.221120
286.495720	11660.492458	28.226138
286.715229	11683.811021	28.231156
286.780461	11699.175312	28.236173
287.340261	11712.829958	28.241191
287.491917	11733.589696	28.246208
287.941691	11757.338264	28.251226
288.395859	11775.548760	28.256244
288.424768	11782.567379	28.261261
288.718477	11796.281897	28.266279
288.974483	11815.874129	28.271296
289.112760	11833.438894	28.276314
289.651148	11840.273933	28.281332
289.465942	11866.136922	28.286349
290.033039	11884.237452	28.291367
290.436647	11897.320873	28.296384
290.523707	11931.341028	28.301402
290.820904	11936.263589	28.306420
291.058598	11963.331573	28.311437
291.619146	11983.379440	28.316455
291.287979	12000.491034	28.321472
291.905693	12019.977945	28.326490
292.418984	12038.191558	28.331508
292.616870	12055.010783	28.336525
292.927987	12069.661847	28.341543
293.347097	12090.560570	28.346560
293.964259	12109.938949	28.351578
294.183019	12125.946388	28.356596
294.220482	12139.963624	28.361613
294.867733	12142.176170	28.366631
295.133391	12172.065356	28.371648
295.221666	12179.184630	28.376666
295.660866	12187.214967	28.381684
295.365313	12210.225578	28.386701
295.956325	12224.852517	28.391719
296.517558	12251.073202	28.396736
296.776551	12265.361171	28.401754
296.788912	12269.194790	28.406772
297.035347	12286.863484	28.411789
297.495092	12309.276464	28.416807
297.736942	12326.230521	28.421824
298.250340	12347.342469	28.426842
298.573939	12352.517654	28.431860
298.852885	12381.922814	28.436877
299.140932	12378.060012	28.441895
299.300034	12392.025815	28.446912
299.556699	12416.073634	28.451930
299.957557	12423.781079	28.456948
299.978981	12451.722460	28.461965
300.571404	12455.934451	28.466983
300.392064	12480.875561	28.472000
300.864113	12495.836035	28.477018
301.308929	12506.398033	28.482036
301.333947	12532.726838	28.487053
301.842100	12538.014941	28.492071
301.896231	12565.098552	28.497088
302.033395	12583.409705	28.502106
302.658599	12605.182689	28.507124
302.741156	12625.441266	28.512141
303.068162	12646.543482	28.517159
303.339383	12670.102318	28.522176
303.362129	12691.730871	28.527194
303.850263	12715.225504	28.532212
304.164261	12739.116178	28.537229
304.642122	12757.900637	28.542247
304.919276	12783.970641	28.547264
304.877404	12810.101370	28.552282
305.643666	12822.700021	28.557300
305.923936	12858.740391	28.562317
306.566056	12861.930955	28.567335
306.652701	12890.530480	28.572352
307.161377	12905.746872	28.577370
307.819581	12918.905598	28.582388
307.745316	12933.600743	28.587405
308.161459	12952.189198	28.592423
308.519462	12966.100511	28.597440
308.676954	12985.395277	28.602458
309.031390	13006.149869	28.607476
309.468294	13027.934101	28.612493
309.843810	13044.535840	28.617511
310.200942	13055.301821	28.622528
310.019058	13068.115905	28.627546
310.385574	13090.052129	28.632564
310.637961	13112.626614	28.637581
311.130608	13132.349893	28.642599
311.604101	13155.868074	28.647616
311.750607	13176.483945	28.652634
312.484209	13187.042717	28.657652
312.558870	13213.845067	28.662669
312.655463	13226.896854	28.667687
313.295774	13249.475088	28.672704
312.954263	13274.211010	28.677722
313.700500	13285.911895	28.682740
314.025505	13312.795897	28.687757
314.029022	13333.065283	28.692775
314.573932	13347.548002	28.697792
315.009025	13380.722452	28.702810
315.471044	13382.682163	28.707828
315.644809	13401.442054	28.712845
315.899453	13420.450189	28.717863
316.306844	13430.134870	28.722880
316.615080	13449.539193	28.727898
316.607109	13471.088761	28.732916
316.735066	13499.696700	28.737933
317.045394	13515.294783	28.742951
317.585609	13545.848662	28.747968
317.375238	13570.834395	28.752986
318.236135	13587.999352	28.758004
318.362851	13620.884918	28.763021
318.523351	13638.031893	28.768039
319.496285	13665.732764	28.773056
319.395713	13696.489119	28.778074
319.929532	13707.363400	28.783092
320.008382	13729.901271	28.788109
320.454893	13758.094458	28.793127
320.693096	13777.274363	28.798144
320.779896	13793.516468	28.803162
321.854518	13805.448635	28.808180
321.930476	13827.260581	28.813197
322.232622	13848.243966	28.818215
322.708941	13854.756025	28.823232
322.549213	13871.825439	28.828250
323.252171	13891.680311	28.833268
323.474803	13914.977916	28.838285
323.337571	13929.098100	28.843303
324.167919	13942.776045	28.848320
324.171796	13977.991522	28.853338
324.595821	13983.743193	28.858356
324.791084	14007.950094	28.863373
325.186910	14029.443021	28.868391
325.564701	14051.755342	28.873408
325.522607	14090.994383	28.878426
326.153051	14092.669414	28.883444
326.539486	14129.512979	28.888461
327.052597	14148.646243	28.893479
327.417718	14167.006550	28.898496
327.306189	14194.556843	28.903514
327.981599	14205.562477	28.908532
328.467471	14239.303945	28.913549
328.606801	14247.662323	28.918567
328.745770	14270.619671	28.923584
329.144089	14297.612940	28.928602
329.630212	14311.337136	28.933620
329.408396	14346.935915	28.938637
330.207151	14371.320856	28.943655
330.846027	14392.504528	28.948672
331.063137	14413.326194	28.953690
331.434358	14432.199584	28.958708
331.989869	14445.879313	28.963725
331.996869	14474.608266	28.968743
332.455459	14485.668888	28.973760
332.776916	14509.841461	28.978778
333.390710	14524.969474	28.983796
333.621052	14546.507807	28.988813
334.005415	14561.128505	28.993831
334.345561	14568.487677	28.998848
334.293868	14600.389747	29.003866
334.673215	14608.081305	29.008884
335.147943	14636.220904	29.013901
335.149788	14658.230624	29.018919
335.630702	14672.368921	29.023936
335.893292	14707.653471	29.028954
336.310794	14729.243025	29.033972
336.427190	14755.591805	29.038989
337.078420	14772.627228	29.044007
337.573112	14794.804584	29.049024
337.826587	14819.151203	29.054042
338.427234	14832.506990	29.059060
338.409854	14863.842801	29.064077
338.649307	14879.892075	29.069095
339.179648	14902.679934	29.074112
339.430696	14927.514132	29.079130
340.083692	14935.344960	29.084148
340.214871	14955.429732	29.089165
340.513510	14981.460284	29.094183
340.811035	14981.232982	29.099200
341.133928	15011.400019	29.104218
341.199599	15032.045792	29.109236
341.877139	15066.579977	29.114253
342.212296	15091.424144	29.119271
342.700521	15098.989162	29.124288
342.623719	15131.083976	29.129306
343.126221	15150.078318	29.134324
343.449299	15167.995934	29.139341
343.514198	15200.032754	29.144359
344.318769	15212.196643	29.149376
344.403023	15232.316314	29.154394
344.670290	15246.003441	29.159412
345.126652	15264.966150	29.164429
345.478091	15297.091283	29.169447
345.955674	15313.769856	29.174464
345.805282	15340.297701	29.179482
346.305163	15357.688198	29.184500
346.560388	15382.598048	29.189517
346.955946	15402.502485	29.194535
347.502850	15435.851734	29.199552
347.614311	15468.254920	29.204570
347.870221	15489.415132	29.209588
348.443786	15501.059508	29.214605
348.429880	15534.478132	29.219623
348.937151	15564.480119	29.224640
348.904455	15592.670663	29.229658
349.368640	15615.768360	29.234676
349.804197	15660.204395	29.239693
350.438809	15692.757864	29.244711
350.936332	15709.750352	29.249728
351.435948	15743.059189	29.254746
351.906980	15765.695716	29.259764
352.208628	15781.131897	29.264781
352.352741	15815.975033	29.269799
353.209793	15820.397886	29.274816
353.034990	15859.467659	29.279834
353.509174	15870.309123	29.284852
353.813852	15893.138859	29.289869
354.056179	15921.319124	29.294887
354.532511	15941.207692	29.299904
355.312207	15967.185408	29.304922
355.291744	15987.380075	29.309940
356.044824	16002.582553	29.314957
356.347477	16028.806396	29.319975
356.942732	16036.541707	29.324992
356.928224	16067.997546	29.330010
357.391048	16073.866483	29.335028
357.920925	16101.764609	29.340045
357.868488	16127.599731	29.345063
358.642909	16145.462628	29.350080
358.588845	16173.124936	29.355098
358.671687	16196.835089	29.360116
359.344123	16222.603983	29.365133
359.680785	16244.905603	29.370151
360.190423	16268.660289	29.375168
360.353023	16297.226383	29.380186
360.439107	16321.615538	29.385204
361.087111	16342.407739	29.390221
361.095944	16377.950658	29.395239
361.656079	16406.659213	29.400256
361.962132	16434.617013	29.405274
362.130912	16459.411968	29.410292
362.576044	16486.040122	29.415309
362.875900	16520.674546	29.420327
363.854955	16538.864969	29.425344
364.236891	16565.577795	29.430362
364.518867	16589.293384	29.435380
364.616208	16611.485362	29.440397
364.773693	16644.133864	29.445415
365.434690	16662.197367	29.450432
365.402021	16695.613561	29.455450
366.010571	16715.359810	29.460468
366.428517	16753.327924	29.465485
366.794151	16784.942891	29.470503
367.183747	16808.845901	29.475520
367.509056	16830.005805	29.480538
367.886883	16857.367638	29.485556
367.908731	16873.191628	29.490573
368.224902	16906.920944	29.495591
368.717358	16928.639695	29.500608
368.834265	16960.482165	29.505626
369.260663	16985.656145	29.510644
369.892152	17024.016717	29.515661
369.949967	17051.315186	29.520679
370.856806	17061.426935	29.525696
371.115986	17098.775829	29.530714
371.446415	17113.306841	29.535732
371.978786	17143.726848	29.540749
372.282613	17177.802396	29.545767
372.899890	17192.831413	29.550784
373.254647	17218.429025	29.555802
373.504245	17243.785561	29.560820
373.943677	17254.340495	29.565837
373.815844	17291.219496	29.570855
374.643718	17315.583505	29.575872
374.860939	17348.628626	29.580890
374.921201	17377.492531	29.585908
375.383991	17398.666665	29.590925
375.478797	17433.655355	29.595943
376.544030	17470.581638	29.600960
376.432047	17504.208052	29.605978
376.813286	17529.946787	29.610996
377.590077	17559.851046	29.616013
378.045680	17598.634572	29.621031
378.620939	17615.860498	29.626048
378.883427	17647.897731	29.631066
379.165413	17666.047129	29.636084
379.586566	17693.299132	29.641101
379.788900	17727.824531	29.646119
380.312426	17748.207179	29.651136
380.551754	17777.321161	29.656154
381.102608	17809.653057	29.661172
381.687630	17820.250466	29.666189
381.768740	17857.947391	29.671207
382.213704	17882.358265	29.676224
382.648607	17913.068530	29.681242
382.871793	17947.956659	29.686260
383.264337	17963.138647	29.691277
383.440466	18000.637307	29.696295
384.124391	18033.756310	29.701312
384.601859	18055.893615	29.706330
384.973379	18096.867660	29.711348
385.240625	18117.398794	29.716365
385.423046	18150.958873	29.721383
386.200376	18173.239031	29.726400
386.458147	18214.839112	29.731418
386.676288	18234.375913	29.736436
387.233691	18257.777161	29.741453
387.486036	18290.987018	29.746471
388.134341	18319.794649	29.751488
388.333108	18347.443955	29.756506
388.853523	18372.101597	29.761524
389.411892	18399.481811	29.766541
389.323278	18427.722681	29.771559
389.783228	18460.291588	29.776576
390.477907	18494.571570	29.781594
390.424513	18525.519844	29.786612
390.974859	18556.916865	29.791629
391.231592	18583.008890	29.796647
392.136811	18618.758224	29.801664
392.584513	18639.384678	29.806682
392.665663	18665.050292	29.811700
392.970157	18689.070988	29.816717
393.448417	18714.202748	29.821735
393.648228	18745.071688	29.826752
394.196649	18775.090027	29.831770
394.449775	18805.217195	29.836788
394.971938	18823.102672	29.841805
394.990815	18851.744236	29.846823
395.352433	18871.814537	29.851840
395.909420	18901.322481	29.856858
396.118707	18944.359124	29.861876
396.749042	18954.118952	29.866893
397.230479	18993.623485	29.871911
397.351220	19029.758919	29.876928
397.884387	19060.700972	29.881946
397.970923	19092.748029	29.886964
398.962047	19121.569680	29.891981
398.817239	19161.938126	29.896999
399.345643	19194.832935	29.902016
399.793419	19223.684775	29.907034
400.216577	19261.082323	29.912052
400.905203	19293.419524	29.917069
400.927255	19323.481817	29.922087
401.871897	19351.824412	29.927104
402.143645	19383.311661	29.932122
402.490078	19414.591119	29.937140
403.181391	19443.830276	29.942157
403.051931	19477.554991	29.947175
403.327881	19500.921007	29.952192
404.094602	19540.046968	29.957210
404.374863	19566.789326	29.962228
405.011451	19603.389268	29.967245
405.302138	19633.828599	29.972263
405.733778	19661.272848	29.977280
406.276513	19689.744016	29.982298
406.588664	19729.365012	29.987316
407.392177	19752.070203	29.992333
407.769987	19788.390179	29.997351
408.058940	19817.471128	30.002368
408.596250	19841.551122	30.007386
408.727509	19869.594070	30.012404
409.271512	19899.034979	30.017421
409.492228	19921.428513	30.022439
409.990730	19955.907927	30.027456
410.526114	19975.086828	30.032474
410.502387	20016.361170	30.037492
411.082009	20042.649561	30.042509
411.406192	20085.622823	30.047527
412.016461	20121.881403	30.052544
412.217842	20144.976869	30.057562
412.745498	20186.901384	30.062580
413.096792	20219.799139	30.067597
413.485141	20252.474830	30.072615
413.753773	20282.483843	30.077632
414.509363	20319.377826	30.082650
415.010661	20355.555617	30.087668
415.149693	20383.812558	30.092685
415.576718	20416.691859	30.097703
416.070580	20452.319269	30.102720
416.485760	20486.692161	30.107738
417.143986	20515.186612	30.112756
417.677233	20533.486743	30.117773
417.751885	20572.054842	30.122791
417.866924	20599.281836	30.127808
418.560816	20629.028741	30.132826
418.836231	20670.822775	30.137844
419.358104	20701.251009	30.142861
419.374200	20734.274614	30.147879
419.792643	20779.695213	30.152896
420.604408	20809.810790	30.157914
420.744688	20842.416737	30.162932
421.521188	20866.373479	30.167949
421.903575	20904.438908	30.172967
422.164682	20929.414423	30.177984
423.063528	20963.578961	30.183002
423.147522	20993.591417	30.188020
423.601096	21014.719636	30.193037
424.202775	21044.889322	30.198055
424.028944	21079.032946	30.203072
424.795712	21096.667524	30.208090
425.010077	21132.872397	30.213108
425.787042	21156.635544	30.218125
425.900191	21193.926299	30.223143
426.656528	21219.707973	30.228160
426.930937	21258.734939	30.233178
427.057783	21293.969199	30.238196
427.418345	21332.207913	30.243213
427.971077	21363.220351	30.248231
428.194768	21407.672078	30.253248
428.667621	21440.835912	30.258266
429.002667	21484.504702	30.263284
429.810630	21520.292097	30.268301
430.221039	21553.641503	30.273319
430.589941	21599.707932	30.278336
431.050179	21630.584801	30.283354
431.292026	21668.785583	30.288372
431.856450	21703.355426	30.293389
432.431113	21732.321447	30.298407
432.679824	21779.302273	30.303424
433.456964	21817.077381	30.308442
433.503368	21850.522299	30.313460
434.075572	21888.497040	30.318477
434.566119	21938.981282	30.323495
434.954771	21976.073645	30.328512
435.640420	22000.843310	30.333530
436.105035	22051.956583	30.338548
436.806189	22077.371852	30.343565
437.116279	22115.095619	30.348583
437.297243	22142.810878	30.353600
437.787907	22167.087983	30.358618
437.599629	22215.112058	30.363636
438.804461	22257.033727	30.368653
439.215709	22289.307490	30.373671
439.249088	22328.430420	30.378688
440.117029	22357.632806	30.383706
440.346593	22402.002599	30.388724
440.913151	22443.456394	30.393741
441.748627	22475.519973	30.398759
441.843670	22502.871601	30.403776
442.516246	22543.978542	30.408794
442.626505	22580.714630	30.413812
443.253597	22617.234393	30.418829
443.920408	22637.362758	30.423847
444.220546	22677.404217	30.428864
445.194744	22709.450014	30.433882
444.840634	22746.648054	30.438900
445.142041	22782.053625	30.443917
445.477231	22810.698446	30.448935
445.925572	22867.496688	30.453952
446.525182	22890.542622	30.458970
446.873514	22929.323097	30.463988
447.350454	22979.073137	30.469005
448.077607	23009.116762	30.474023
448.230675	23051.791583	30.479040
448.960587	23081.175746	30.484058
449.351731	23131.806136	30.489076
449.693760	23159.849622	30.494093
450.329039	23194.395014	30.499111
450.234690	23239.117046	30.504128
450.896160	23262.427628	30.509146
451.395171	23309.437495	30.514164
451.883120	23334.377441	30.519181
452.452533	23376.842258	30.524199
452.513268	23398.814300	30.529216
453.403476	23433.541913	30.534234
453.663390	23476.547036	30.539252
454.027326	23510.406284	30.544269
454.270744	23538.294828	30.549287
454.904908	23584.303822	30.554304
455.545338	23612.673982	30.559322
455.998234	23655.266005	30.564340
456.043753	23686.871247	30.569357
456.673940	23734.283197	30.574375
456.781583	23776.439073	30.579392
457.381395	23817.778753	30.584410
457.870850	23866.356066	30.589428
458.242366	23911.439582	30.594445
458.806851	23948.461420	30.599463
459.600304	24006.141483	30.604480
460.008682	24034.695827	30.609498
460.369157	24081.494202	30.614516
461.038123	24119.082599	30.619533
461.492293	24157.690656	30.624551
461.989431	24200.877547	30.629568
462.297051	24238.428229	30.634586
462.994597	24277.314834	30.639604
463.275516	24322.720361	30.644621
463.676784	24351.194406	30.649639
464.332152	24397.578985	30.654656
464.620774	24433.713942	30.659674
465.542656	24487.677889	30.664692
465.879266	24519.033064	30.669709
466.339528	24555.464739	30.674727
466.491575	24585.333491	30.679744
467.331467	24626.890879	30.684762
467.930177	24674.436808	30.689780
467.927014	24707.728365	30.694797
468.438483	24743.139515	30.699815
468.577390	24797.076298	30.704832
469.485092	24834.841241	30.709850
469.841248	24885.181401	30.714868
470.221738	24928.540825	30.719885
470.674272	24961.836320	30.724903
471.408211	25011.966095	30.729920
471.826875	25060.463888	30.734938
472.029857	25103.310619	30.739956
472.531881	25145.060800	30.744973
473.278942	25183.313598	30.749991
473.513921	25235.062656	30.755008
474.090622	25267.723139	30.760026
474.693001	25311.986753	30.765044
475.145727	25356.839842	30.770061
476.132603	25402.087249	30.775079
476.304408	25439.435934	30.780096
476.903280	25479.915537	30.785114
477.562982	25520.776291	30.790132
477.540860	25557.062813	30.795149
478.348657	25585.162526	30.800167
478.436576	25630.698075	30.805184
479.253906	25673.450876	30.810202
479.513225	25712.151452	30.815220
479.894056	25755.670619	30.820237
480.667955	25789.434992	30.825255
480.986208	25828.514050	30.830272
481.261555	25878.577143	30.835290
481.802054	25917.061321	30.840308
482.225518	25957.211486	30.845325
482.955829	25993.579446	30.850343
483.064163	26026.889801	30.855360
483.622103	26070.765280	30.860378
483.686979	26103.108294	30.865396
484.209361	26155.948111	30.870413
484.693677	26199.814021	30.875431
485.405534	26245.777876	30.880448
485.817557	26289.372086	30.885466
486.275298	26341.860420	30.890484
486.700771	26373.390380	30.895501
487.246276	26421.101353	30.900519
487.725158	26473.693838	30.905536
488.087856	26516.265302	30.910554
488.673986	26559.336146	30.915572
489.145107	26612.024967	30.920589
489.559615	26658.581681	30.925607
490.088016	26708.406577	30.930624
490.472887	26754.476364	30.935642
490.895675	26812.949551	30.940660
491.545131	26862.710699	30.945677
492.079890	26909.626724	30.950695
492.758427	26964.884724	30.955712
492.901595	27002.973363	30.960730
493.830763	27051.584705	30.965748
494.255489	27100.582485	30.970765
494.821634	27144.875728	30.975783
495.345483	27195.551340	30.980800
495.667700	27243.377236	30.985818
495.948670	27300.948109	30.990836
496.347634	27346.307369	30.995853
496.803128	27393.297755	31.000871
497.346828	27455.626882	31.005888
497.979950	27502.203316	31.010906
498.900112	27560.028902	31.015924
499.212896	27604.734328	31.020941
500.140040	27648.155240	31.025959
500.486274	27701.650377	31.030976
500.933784	27743.971074	31.035994
501.268772	27790.689098	31.041012
501.650908	27848.298673	31.046029
502.288837	27895.610395	31.051047
503.019692	27943.604045	31.056064
503.302162	27995.568017	31.061082
504.330539	28037.828016	31.066100
504.565498	28079.134197	31.071117
504.934412	28122.099753	31.076135
505.518258	28169.847052	31.081152
505.808718	28216.586206	31.086170
506.426915	28266.482740	31.091188
506.821264	28324.792215	31.096205
507.358642	28364.623103	31.101223
507.694850	28413.191261	31.106240
508.539155	28483.723946	31.111258
509.146584	28524.695090	31.116276
509.548178	28582.269170	31.121293
509.973136	28632.741347	31.126311
510.517320	28677.143082	31.131328
511.024839	28727.702825	31.136346
511.530876	28775.713887	31.141364
512.269632	28822.194352	31.146381
512.963701	28865.404489	31.151399
513.594024	28912.799105	31.156416
513.943540	28958.811176	31.161434
514.283988	28991.066642	31.166452
514.842540	29053.048843	31.171469
515.395245	29088.563024	31.176487
515.712852	29128.413093	31.181504
516.062738	29186.660240	31.186522
516.849365	29223.470499	31.191540
517.202177	29279.048447	31.196557
517.444385	29311.800303	31.201575
518.043852	29362.488639	31.206592
518.382872	29419.463780	31.211610
519.129813	29456.628137	31.216628
519.199230	29511.695295	31.221645
520.111814	29542.822295	31.226663
520.384651	29603.355128	31.231680
520.892648	29654.838716	31.236698
521.921065	29694.654489	31.241716
521.981620	29754.838064	31.246733
522.713990	29805.631891	31.251751
522.939405	29852.329390	31.256768
523.476550	29909.705575	31.261786
523.920060	29956.749019	31.266804
524.011988	30037.028920	31.271821
524.695620	30068.633288	31.276839
525.353595	30142.153442	31.281856
525.457877	30197.961571	31.286874
526.018401	30250.624513	31.291892
526.750786	30321.410290	31.296909
527.114901	30377.485192	31.301927
527.781946	30453.267340	31.306944
528.208976	30512.029866	31.311962
529.051726	30575.017916	31.316980
529.447184	30642.289141	31.321997
530.029912	30698.745371	31.327015
530.921722	30746.732707	31.332032
531.525089	30816.374419	31.337050
532.307515	30871.018649	31.342068
532.571419	30935.368988	31.347085
533.190554	30989.125601	31.352103
533.899402	31049.736405	31.357120
534.273005	31104.414296	31.362138
535.044549	31151.583350	31.367156
535.366434	31223.866834	31.372173
535.738108	31269.000980	31.377191
536.798410	31326.206873	31.382208
537.138701	31381.481166	31.387226
537.956585	31429.293279	31.392244
538.048123	31481.403289	31.397261
538.717932	31535.481331	31.402279
539.268090	31605.683981	31.407296
539.691616	31665.167180	31.412314
540.377158	31717.324746	31.417332
540.710944	31774.633369	31.422349
541.173446	31833.271366	31.427367
542.203290	31897.347018	31.432384
542.540683	31955.911461	31.437402
543.007229	32006.033040	31.442420
543.677232	32064.328243	31.447437
543.881640	32118.759590	31.452455
544.706965	32168.942172	31.457472
544.821714	32233.861484	31.462490
546.019440	32287.456894	31.467508
546.465725	32345.427164	31.472525
547.085277	32407.909637	31.477543
547.641387	32461.943057	31.482560
547.944317	32518.056960	31.487578
548.681099	32562.032735	31.492596
549.004038	32624.931082	31.497613
549.705061	32674.002843	31.502631
550.364744	32732.626966	31.507648
550.738703	32795.302900	31.512666
551.423967	32842.519138	31.517684
552.031710	32900.537082	31.522701
552.276381	32943.714833	31.527719
552.798724	32996.490095	31.532736
553.099919	33057.806329	31.537754
553.953201	33110.798552	31.542772
554.353401	33161.552861	31.547789
555.077649	33210.811596	31.552807
555.661014	33266.130429	31.557824
556.201991	33307.161565	31.562842
556.944720	33360.254869	31.567860
557.155952	33419.567641	31.572877
558.075741	33469.211281	31.577895
558.318200	33520.873132	31.582912
558.894341	33570.845298	31.587930
559.627077	33627.743609	31.592948
560.092359	33693.291864	31.597965
560.572553	33742.646096	31.602983
561.430877	33788.857951	31.608000
561.471575	33853.258946	31.613018
562.594701	33904.615257	31.618036
562.974900	33972.116216	31.623053
563.144372	34023.233033	31.628071
563.461927	34087.781564	31.633088
564.317848	34156.368976	31.638106
564.993973	34213.685613	31.643124
565.209881	34278.885958	31.648141
565.782341	34334.793725	31.653159
566.476309	34410.342163	31.658176
566.802596	34473.505244	31.663194
567.460095	34541.628345	31.668212
567.901896	34609.686405	31.673229
568.573001	34672.073605	31.678247
569.337606	34745.525757	31.683264
569.481227	34811.355389	31.688282
570.294396	34886.876644	31.693300
570.979198	34954.435048	31.698317
571.559108	35012.521260	31.703335
572.484999	35085.193857	31.708352
572.828440	35153.891968	31.713370
573.540078	35214.712164	31.718388
574.087370	35278.254937	31.723405
574.762425	35343.013932	31.728423
575.675081	35402.182497	31.733440
575.881768	35474.663220	31.738458
576.487278	35531.894759	31.743476
577.307275	35599.846655	31.748493
577.902877	35665.860268	31.753511
578.486820	35725.554528	31.758528
578.937020	35786.694486	31.763546
579.852833	35840.956334	31.768564
580.523949	35897.168244	31.773581
580.764475	35962.531577	31.778599
581.741441	36018.036800	31.783616
582.059310	36084.410347	31.788634
582.983393	36138.005787	31.793652
583.296075	36198.008447	31.798669
583.656774	36259.309995	31.803687
584.301217	36320.934073	31.808704
584.730742	36390.875637	31.813722
585.475061	36453.282147	31.818740
585.996280	36511.932074	31.823757
586.647247	36575.522231	31.828775
586.938545	36634.668241	31.833792
587.507832	36698.067190	31.838810
588.155047	36767.671199	31.843828
588.308076	36831.114233	31.848845
589.212809	36901.768203	31.853863
590.315914	36960.566342	31.858880
590.650102	37034.711343	31.863898
591.099470	37090.291369	31.868916
591.352869	37151.692595	31.873933
592.032988	37206.975987	31.878951
592.684033	37269.687965	31.883968
593.368918	37342.870345	31.888986
594.187688	37382.106760	31.894004
594.583603	37447.194078	31.899021
595.097613	37517.132321	31.904039
595.813675	37567.086120	31.909056
596.071173	37646.763602	31.914074
597.149197	37707.487382	31.919092
597.405473	37769.344736	31.924109
597.565672	37833.778031	31.929127
598.471482	37900.802704	31.934144
598.889412	37970.139928	31.939162
599.306469	38043.681924	31.944180
599.985384	38115.558483	31.949197
600.507213	38197.991250	31.954215
601.278565	38263.543343	31.959232
602.027273	38349.013657	31.964250
602.541365	38412.629734	31.969268
603.109561	38486.568324	31.974285
603.763775	38556.705159	31.979303
604.455651	38624.010938	31.984320
604.728426	38707.598308	31.989338
605.804212	38769.724351	31.994356
605.923233	38849.856129	31.999373
606.434984	38942.792675	32.004391
607.933850	39000.556552	32.009408
608.329634	39088.932808	32.014426
608.753358	39156.894137	32.019444
609.603260	39220.425901	32.024461
610.539637	39295.152824	32.029479
611.267841	39355.131866	32.034496
611.359584	39428.932123	32.039514
612.129743	39500.691705	32.044532
612.837848	39571.139180	32.049549
613.375674	39650.999984	32.054567
614.233839	39708.771085	32.059584
614.465189	39776.289871	32.064602
615.207892	39846.802128	32.069620
616.014098	39923.964899	32.074637
616.284975	39995.427049	32.079655
616.987262	40061.120121	32.084672
617.579693	40141.135015	32.089690
617.791998	40209.043668	32.094708
618.949285	40287.955574	32.099725
619.473195	40367.818636	32.104743
620.250103	40429.415740	32.109760
620.868863	40507.792628	32.114778
621.687693	40573.231483	32.119796
622.364291	40651.649924	32.124813
622.788884	40722.353909	32.129831
623.561202	40772.853298	32.134848
623.753943	40862.259771	32.139866
624.645852	40933.300808	32.144884
625.180016	41006.137619	32.149901
625.549652	41079.652268	32.154919
626.936520	41137.324602	32.159936
627.150897	41212.194544	32.164954
628.001632	41285.336820	32.169972
628.778002	41358.052866	32.174989
628.874700	41431.888727	32.180007
629.632846	41504.226363	32.185024
630.361760	41576.225002	32.190042
630.805264	41654.468424	32.195060
631.797761	41704.514046	32.200077
632.284155	41778.094235	32.205095
633.142009	41837.292741	32.210112
633.348003	41900.561426	32.215130
634.098918	41973.170442	32.220148
634.464771	42034.853530	32.225165
634.919871	42110.265024	32.230183
635.830786	42173.566404	32.235200
636.362442	42249.783498	32.240218
637.063164	42314.468236	32.245236
637.590772	42381.306615	32.250253
638.310605	42440.883484	32.255271
638.923242	42509.128988	32.260288
639.407138	42590.530021	32.265306
640.155648	42666.987626	32.270324
640.715198	42732.322301	32.275341
641.243728	42814.743030	32.280359
641.937008	42889.297393	32.285376
642.606772	42963.328680	32.290394
643.165204	43042.692389	32.295412
644.143762	43109.815553	32.300429
644.182217	43189.199602	32.305447
645.328514	43262.821726	32.310464
645.670710	43345.351399	32.315482
646.138227	43431.602164	32.320500
646.709764	43515.130256	32.325517
647.432085	43603.161458	32.330535
648.498613	43674.641912	32.335552
649.101711	43757.243906	32.340570
649.432728	43837.204312	32.345588
650.158752	43922.366309	32.350605
650.827228	44013.284768	32.355623
651.451823	44081.571929	32.360640
652.625008	44165.578048	32.365658
653.261058	44244.520383	32.370676
653.724751	44314.682141	32.375693
654.553698	44413.700240	32.380711
655.498073	44479.602544	32.385728
655.960212	44567.488707	32.390746
656.433187	44638.319536	32.395764
657.628623	44711.231938	32.400781
658.080381	44794.056143	32.405799
658.538506	44865.635474	32.410816
659.406859	44954.431939	32.415834
660.011237	45026.521322	32.420852
660.841246	45096.780121	32.425869
661.293489	45175.365226	32.430887
662.100062	45252.019551	32.435904
662.725293	45330.134611	32.440922
663.110366	45415.931316	32.445940
663.909700	45489.486959	32.450957
664.701082	45571.418448	32.455975
665.607897	45652.077580	32.460992
665.930951	45718.560666	32.466010
666.534090	45801.048475	32.471028
667.667068	45872.696820	32.476045
667.876115	45955.904155	32.481063
668.807553	46028.088515	32.486080
669.578278	46108.712112	32.491098
670.137249	46181.811281	32.496116
671.093291	46253.544023	32.501133
671.248294	46337.990367	32.506151
672.470647	46413.017492	32.511168
672.922194	46488.870314	32.516186
673.452208	46567.776755	32.521204
673.902558	46638.887246	32.526221
674.433350	46730.542628	32.531239
675.319428	46799.661636	32.536256
676.183620	46882.265703	32.541274
676.799027	46964.150221	32.546292
677.492717	47041.692587	32.551309
678.042373	47117.588531	32.556327
678.639075	47181.416679	32.561344
679.266626	47256.921336	32.566362
679.969933	47319.589119	32.571380
680.812442	47401.317946	32.576397
681.159533	47472.401264	32.581415
682.011403	47546.518327	32.586432
682.516699	47639.720267	32.591450
682.656470	47711.580914	32.596468
683.735338	47782.332743	32.601485
684.402561	47863.855693	32.606503
684.849100	47943.031130	32.611520
685.752704	48034.018436	32.616538
686.217718	48113.535758	32.621556
687.326934	48194.197469	32.626573
687.577783	48278.772355	32.631591
688.802208	48368.138576	32.636608
689.388139	48438.589083	32.641626
690.065051	48527.876080	32.646644
690.635260	48615.112514	32.651661
691.350784	48705.120338	32.656679
692.038157	48784.493123	32.661696
693.034928	48864.020343	32.666714
693.566280	48960.853239	32.671732
694.388316	49040.106899	32.676749
694.952897	49126.613867	32.681767
695.939315	49202.809041	32.686784
696.469203	49283.473265	32.691802
697.161567	49372.442643	32.696820
698.138183	49453.908543	32.701837
698.809548	49552.619427	32.706855
699.497268	49629.276290	32.711872
700.212063	49703.007467	32.716890
700.713618	49788.368705	32.721908
701.869052	49867.504298	32.726925
702.621281	49943.115778	32.731943
703.094045	50029.057678	32.736960
703.842471	50108.678503	32.741978
704.283727	50196.429840	32.746996
705.344403	50275.765975	32.752013
705.822024	50361.724343	32.757031
706.229729	50457.422883	32.762048
707.373150	50524.731366	32.767066
707.579216	50620.394578	32.772084
708.565247	50699.220482	32.777101
709.550736	50788.160532	32.782119
709.979878	50882.606832	32.787136
710.767347	50968.270269	32.792154
711.357959	51053.846620	32.797172
712.468491	51139.349980	32.802189
712.929117	51224.203149	32.807207
713.711666	51307.259860	32.812224
714.580129	51390.763880	32.817242
715.557837	51480.826562	32.822260
715.571996	51548.742349	32.827277
716.399878	51633.884012	32.832295
717.194934	51730.510270	32.837312
717.978113	51817.447968	32.842330
718.722327	51901.480132	32.847348
719.356295	51983.521921	32.852365
720.160607	52072.232486	32.857383
721.028957	52152.442030	32.862400
721.850354	52236.248073	32.867418
722.224334	52328.530941	32.872436
723.061609	52407.817984	32.877453
723.780187	52495.514875	32.882471
724.429087	52589.541407	32.887488
725.396452	52664.796221	32.892506
725.975307	52735.617339	32.897524
726.873919	52809.885878	32.902541
727.308610	52887.680966	32.907559
727.915655	52976.472492	32.912576
728.551046	53046.331387	32.917594
729.214220	53138.292250	32.922612
730.126881	53208.592339	32.927629
730.657368	53296.216526	32.932647
731.277678	53374.216605	32.937664
732.367419	53452.057210	32.942682
732.651507	53539.546336	32.947700
733.355575	53633.448708	32.952717
734.348705	53726.741405	32.957735
734.594328	53818.888249	32.962752
735.730903	53910.009928	32.967770
736.493066	54002.520779	32.972788
737.211444	54088.215646	32.977805
737.635039	54182.230213	32.982823
738.527032	54285.841013	32.987840
739.144164	54368.704308	32.992858
739.729780	54476.429451	32.997876
741.095912	54567.200284	33.002893
741.684226	54669.087871	33.007911
741.928659	54757.296619	33.012928
742.840030	54845.193253	33.017946
743.687580	54955.032268	33.022964
744.663627	55049.654614	33.027981
745.162323	55150.946610	33.032999
745.877046	55250.408916	33.038016
746.996052	55343.460969	33.043034
747.650541	55437.500178	33.048052
748.432776	55534.431607	33.053069
749.329246	55630.074556	33.058087
750.054660	55728.096827	33.063104
750.941044	55818.864298	33.068122
751.799364	55914.375915	33.073140
752.745227	56014.783231	33.078157
753.218838	56093.766136	33.083175
753.950545	56188.687085	33.088192
754.984246	56274.187605	33.093210
755.260351	56372.723375	33.098228
756.387168	56463.972174	33.103245
757.298257	56558.031110	33.108263
758.356434	56651.149903	33.113280
759.180041	56738.317473	33.118298
759.402635	56828.763330	33.123316
760.176969	56910.859268	33.128333
761.081463	57006.779226	33.133351
761.599492	57094.877256	33.138368
762.553127	57190.486648	33.143386
763.035781	57289.599417	33.148404
764.061667	57387.832917	33.153421
764.911136	57482.298191	33.158439
765.391569	57576.622732	33.163456
766.387001	57652.972489	33.168474
767.220478	57755.833776	33.173492
768.037436	57848.505133	33.178509
768.715896	57939.348235	33.183527
769.486262	58047.384426	33.188544
770.331203	58132.582866	33.193562
771.035122	58218.493821	33.198580
771.710659	58309.143172	33.203597
772.621068	58408.373979	33.208615
772.988972	58501.261651	33.213632
774.162918	58593.194878	33.218650
774.790086	58694.862765	33.223668
775.301041	58783.664534	33.228685
776.488898	58876.323517	33.233703
776.892386	58962.230457	33.238720
777.558493	59035.821331	33.243738
778.438241	59143.611476	33.248756
779.017309	59219.385107	33.253773
780.173496	59314.756227	33.258791
780.392013	59409.992174	33.263808
781.502334	59490.482065	33.268826
782.059284	59591.458247	33.273844
782.884955	59684.661159	33.278861
783.463155	59771.383192	33.283879
784.128226	59881.178293	33.288896
785.183990	59969.427473	33.293914
785.819912	60078.400534	33.298932
786.662312	60174.472252	33.303949
787.310733	60276.688098	33.308967
787.963532	60392.131889	33.313984
789.023873	60490.140953	33.319002
789.585401	60592.872057	33.324020
790.334510	60698.208212	33.329037
791.318258	60807.077083	33.334055
791.875761	60909.835732	33.339072
792.876773	61025.231836	33.344090
793.678295	61127.730008	33.349108
794.374785	61235.473080	33.354125
795.354949	61340.843862	33.359143
795.951910	61455.266345	33.364160
796.918606	61562.321755	33.369178
797.707042	61672.668632	33.374196
798.349269	61779.058294	33.379213
799.175965	61885.417998	33.384231
799.953123	62002.139732	33.389248
800.995826	62099.773877	33.394266
801.771774	62222.027692	33.399284
802.773626	62321.357290	33.404301
803.560318	62434.552907	33.409319
804.087546	62545.617687	33.414336
805.235317	62653.066018	33.419354
806.348152	62758.845644	33.424372
806.869313	62872.871384	33.429389
807.492265	62984.504227	33.434407
808.237502	63089.758499	33.439424
809.484341	63194.658540	33.444442
810.355734	63307.863911	33.449460
810.764388	63416.999779	33.454477
811.795453	63524.851224	33.459495
812.402816	63643.317054	33.464512
813.326828	63754.341677	33.469530
814.202821	63867.498780	33.474548
815.034432	63975.834374	33.479565
815.969542	64069.108668	33.484583
817.125940	64184.762298	33.489600
817.556303	64293.071093	33.494618
818.306635	64406.378348	33.499636
818.955459	64512.199440	33.504653
820.017797	64620.803671	33.509671
820.907543	64740.891615	33.514688
821.601695	64829.948471	33.519706
822.522412	64950.538227	33.524724
823.192254	65063.464113	33.529741
824.251673	65171.730334	33.534759
824.965490	65280.028990	33.539776
826.011367	65394.095594	33.544794
826.735578	65505.080431	33.549812
827.533882	65606.962871	33.554829
828.831379	65709.989680	33.559847
829.077649	65830.259858	33.564864
830.192108	65931.440440	33.569882
830.775421	66035.206513	33.574900
831.504545	66132.374160	33.579917
832.403465	66227.933681	33.584935
833.195620	66337.097285	33.589952
833.857934	66423.700616	33.594970
834.765717	66533.724882	33.599988
835.579866	66644.662948	33.605005
836.010288	66749.924567	33.610023
836.662863	66854.347057	33.615040
837.901124	66967.789805	33.620058
838.516955	67074.394299	33.625076
839.134075	67198.752033	33.630093
839.735561	67304.512879	33.635111
840.358444	67431.842513	33.640128
841.749287	67547.387452	33.645146
842.727377	67661.332172	33.650164
843.227713	67788.532486	33.655181
844.491833	67899.080289	33.660199
845.081824	68031.261989	33.665216
845.896960	68143.674597	33.670234
847.038967	68269.304845	33.675252
847.953333	68392.545598	33.680269
848.964352	68499.913860	33.685287
849.433778	68623.197925	33.690304
850.407449	68742.953425	33.695322
850.938057	68872.229082	33.700340
851.793066	68994.446210	33.705357
853.339122	69113.843578	33.710375
854.057300	69234.010820	33.715392
854.977032	69364.407488	33.720410
855.609709	69473.152075	33.725428
856.218372	69593.775739	33.730445
857.102466	69724.199466	33.735463
858.047308	69849.580791	33.740480
859.141751	69968.754129	33.745498
860.133962	70099.927361	33.750516
861.158973	70229.477242	33.755533
862.087628	70339.049880	33.760551
862.670704	70461.794614	33.765568
863.426326	70579.933466	33.770586
864.221972	70697.275936	33.775604
864.965109	70823.929363	33.780621
865.975006	70962.490607	33.785639
867.070052	71098.781199	33.790656
868.120728	71217.235192	33.795674
868.885366	71333.131863	33.800692
869.658737	71467.846528	33.805709
870.459373	71582.726822	33.810727
871.561193	71719.538751	33.815744
872.173068	71838.441816	33.820762
873.183679	71967.024374	33.825780
873.744604	72091.514737	33.830797
875.158478	72204.829820	33.835815
875.589364	72342.420639	33.840832
876.758018	72462.626285	33.845850
877.604493	72604.089774	33.850868
878.361293	72729.854124	33.855885
879.561938	72842.480556	33.860903
880.099782	72977.464897	33.865920
881.053037	73108.428871	33.870938
882.107430	73234.058385	33.875956
882.866112	73357.005524	33.880973
883.742600	73479.326760	33.885991
884.727968	73611.983312	33.891008
885.626156	73738.457381	33.896026
886.246206	73853.398523	33.901044
887.240704	73990.995085	33.906061
888.099520	74108.244382	33.911079
888.542933	74246.787468	33.916096
889.511390	74385.086490	33.921114
890.534726	74488.156663	33.926132
891.372500	74614.241019	33.931149
892.319636	74737.120478	33.936167
893.327575	74868.516013	33.941184
893.751049	74979.447876	33.946202
894.844506	75118.616283	33.951220
895.280355	75243.815704	33.956237
896.517439	75370.021773	33.961255
897.148101	75505.170776	33.966272
898.170132	75640.104092	33.971290
899.006495	75763.905710	33.976308
899.718097	75893.098417	33.981325
900.667683	76023.884332	33.986343
901.381530	76176.771211	33.991360
902.191169	76308.239738	33.996378
903.325515	76455.581615	34.001396
903.925623	76605.340423	34.006413
905.127280	76748.473306	34.011431
905.818178	76896.100167	34.016448
906.428512	77041.761562	34.021466
907.837321	77181.959742	34.026484
908.596217	77336.358866	34.031501
909.781336	77465.501390	34.036519
910.739576	77620.135175	34.041536
912.017217	77766.336132	34.046554
912.945908	77901.817302	34.051572
913.666113	78049.491227	34.056589
914.563699	78186.440436	34.061607
915.682891	78324.834004	34.066624
916.696686	78472.759466	34.071642
917.275369	78604.425210	34.076660
918.551671	78753.700741	34.081677
919.695835	78886.356306	34.086695
920.641516	79038.319875	34.091712
921.164541	79181.896848	34.096730
922.594898	79319.625165	34.101748
923.029529	79466.039861	34.106765
924.102305	79600.488994	34.111783
925.073579	79747.215300	34.116800
925.644643	79892.079328	34.121818
926.768302	80031.684578	34.126836
927.536955	80182.672969	34.131853
928.779103	80325.809336	34.136871
929.666052	80479.658500	34.141888
930.508308	80629.264928	34.146906
931.784690	80770.816907	34.151924
932.108269	80916.759570	34.156941
933.368113	81073.935624	34.161959
934.388380	81213.122400	34.166976
935.286889	81353.355028	34.171994
936.421109	81502.634230	34.177012
936.868788	81660.524331	34.182029
937.912193	81805.404681	34.187047
939.023782	81962.877087	34.192064
940.149625	82113.351048	34.197082
940.964432	82245.732758	34.202100
942.016909	82402.237338	34.207117
943.175747	82538.739430	34.212135
943.978239	82678.825237	34.217152
945.072695	82826.980840	34.222170
946.073704	82958.361549	34.227188
947.049404	83116.876629	34.232205
947.430118	83249.247326	34.237223
948.920986	83392.652809	34.242240
949.918550	83530.813470	34.247258
950.735174	83676.154368	34.252276
951.582317	83818.061886	34.257293
952.720208	83955.796954	34.262311
953.326376	84084.275643	34.267328
954.283203	84215.594886	34.272346
955.507099	84345.124413	34.277364
956.058837	84479.865536	34.282381
957.180886	84612.798452	34.287399
958.136117	84753.706774	34.292416
958.943319	84898.645618	34.297434
959.950139	85028.417324	34.302452
960.693986	85177.664653	34.307469
961.947153	85315.103987	34.312487
962.626953	85463.857543	34.317504
963.504237	85607.093439	34.322522
964.670756	85752.009806	34.327540
965.370994	85901.800486	34.332557
966.269806	86050.920197	34.337575
967.262500	86191.508291	34.342592
967.617080	86352.021123	34.347610
968.758227	86499.116710	34.352628
969.919698	86675.311377	34.357645
971.210685	86827.629987	34.362663
972.256242	86978.515771	34.367680
973.324956	87142.503815	34.372698
974.436537	87291.975888	34.377716
975.375784	87453.905604	34.382733
976.357304	87591.156389	34.387751
977.465443	87749.003924	34.392768
978.070183	87908.106453	34.397786
979.159519	88053.499048	34.402804
980.005351	88226.504800	34.407821
980.930108	88375.894372	34.412839
982.251635	88541.166576	34.417856
982.800276	88707.377753	34.422874
984.135854	88861.246191	34.427892
984.887597	89031.912870	34.432909
986.208907	89186.424938	34.437927
987.015344	89348.554065	34.442944
987.785868	89521.012100	34.447962
989.224880	89672.077769	34.452980
990.031731	89837.614924	34.457997
991.091985	90000.668451	34.463015
992.189432	90163.020776	34.468032
992.971320	90325.439033	34.473050
994.304069	90490.627924	34.478068
995.260760	90649.494318	34.483085
995.978945	90820.907092	34.488103
997.064377	90978.830350	34.493120
997.651508	91149.191205	34.498138
999.266489	91305.332870	34.503156
1000.199463	91482.626133	34.508173
1001.031185	91645.291864	34.513191
1002.159719	91812.048876	34.518208
1002.933572	91985.441720	34.523226
1004.128680	92146.601339	34.528244
1005.233472	92311.283384	34.533261
1005.923601	92482.870782	34.538279
1007.336192	92641.117871	34.543296
1008.130454	92814.981620	34.548314
1009.254909	92975.012778	34.553332
1010.191656	93134.500035	34.558349
1011.480052	93310.437636	34.563367
1012.446668	93477.049255	34.568384
1012.926829	93643.932328	34.573402
1014.128545	93811.159295	34.578420
1014.892770	93986.251620	34.583437
1016.230096	94150.097392	34.588455
1017.168153	94322.422580	34.593472
1018.189234	94487.557198	34.598490
1019.063001	94639.038391	34.603508
1020.017773	94810.604639	34.608525
1021.021073	94960.692792	34.613543
1022.417849	95122.591893	34.618560
1023.068071	95277.633445	34.623578
1023.945061	95437.588601	34.628596
1025.131119	95602.133673	34.633613
1026.065939	95760.929267	34.638631
1027.136990	95925.343570	34.643648
1028.239738	96105.655326	34.648666
1029.168001	96263.670259	34.653684
1030.267966	96439.800564	34.658701
1031.087954	96596.696045	34.663719
1032.113632	96775.221221	34.668736
1032.601462	96944.467499	34.673754
1034.262013	97112.324554	34.678772
1035.022696	97309.952210	34.683789
1035.969618	97486.355741	34.688807
1037.323327	97650.525741	34.693824
1038.175836	97840.969763	34.698842
1039.144812	98013.100119	34.703860
1040.597554	98192.628323	34.708877
1041.625053	98372.588970	34.713895
1042.629288	98550.275629	34.718912
1043.752461	98734.705294	34.723930
1044.689883	98899.446057	34.728948
1046.144551	99086.083624	34.733965
1046.865316	99256.794684	34.738983
1048.032848	99437.100605	34.744000
1049.228816	99620.290104	34.749018
1050.414602	99794.460662	34.754036
1051.209342	99975.750053	34.759053
1052.322672	100159.634529	34.764071
1053.441458	100332.458611	34.769088
1053.948333	100525.582078	34.774106
1055.346129	100702.363949	34.779124
1056.488261	100892.865251	34.784141
1057.280207	101076.435884	34.789159
1058.542745	101263.304738	34.794176
1059.694756	101448.420375	34.799194
1061.037980	101642.281380	34.804212
1062.061763	101819.430351	34.809229
1062.734517	101999.487851	34.814247
1064.141931	102190.056186	34.819264
1065.167683	102379.175720	34.824282
1066.224245	102559.882822	34.829300
1067.266542	102741.923240	34.834317
1068.122183	102926.775520	34.839335
1069.438518	103114.972226	34.844352
1070.573817	103304.365318	34.849370
1071.784783	103488.213027	34.854388
1072.626824	103685.610475	34.859405
1073.740919	103864.816395	34.864423
1074.823637	104055.642032	34.869440
1075.783054	104246.160164	34.874458
1077.048840	104423.939063	34.879476
1078.478559	104614.610076	34.884493
1079.140426	104807.435790	34.889511
1080.543555	104986.284956	34.894528
1081.385087	105176.512689	34.899546
1082.536039	105343.374227	34.904564
1083.671754	105536.304233	34.909581
1084.729287	105720.800846	34.914599
1086.059318	105898.819699	34.919616
1086.814086	106093.653215	34.924634
1087.842691	106268.026071	34.929652
1089.027566	106469.402631	34.934669
1089.972807	106647.211467	34.939687
1091.261487	106817.441238	34.944704
1092.273166	106991.998949	34.949722
1093.298727	107160.374527	34.954740
1094.269664	107341.489545	34.959757
1095.278179	107530.579222	34.964775
1096.154648	107699.616141	34.969792
1097.333312	107887.641576	34.974810
1098.365893	108074.476504	34.979828
1099.389629	108264.455472	34.984845
1100.274504	108446.466146	34.989863
1101.578251	108624.330144	34.994880
1102.775610	108826.456991	34.999898
1103.889380	109012.765655	35.004916
1104.944195	109204.975451	35.009933
1105.749382	109398.025898	35.014951
1107.587399	109587.448855	35.019968
1108.139561	109795.478438	35.024986
1109.324766	109977.513069	35.030004
1110.504211	110176.954798	35.035021
1111.025173	110386.704135	35.040039
1112.111445	110584.124778	35.045056
1113.425775	110784.625378	35.050074
1114.784529	110998.307201	35.055092
1116.131710	111193.117545	35.060109
1117.068795	111403.135219	35.065127
1118.143289	111602.984702	35.070144
1119.395294	111804.605157	35.075162
1120.406242	112009.294633	35.080180
1121.774937	112211.785540	35.085197
1123.025733	112429.005408	35.090215
1124.275415	112614.631984	35.095232
1125.409014	112818.648398	35.100250
1126.442133	113018.616282	35.105268
1127.540382	113229.039217	35.110285
1128.640688	113433.471036	35.115303
1129.727728	113625.516332	35.120320
1130.494228	113838.165082	35.125338
1131.621000	114044.738056	35.130356
1133.070558	114257.669810	35.135373
1133.915835	114478.253983	35.140391
1135.388147	114685.471356	35.145408
1136.792063	114912.085898	35.150426
1137.657455	115112.337157	35.155444
1138.999440	115315.019644	35.160461
1139.931769	115535.927099	35.165479
1141.185394	115739.311397	35.170496
1142.471741	115954.601513	35.175514
1143.738238	116157.213806	35.180532
1145.007193	116362.538547	35.185549
1145.865965	116581.565759	35.190567
1147.186228	116780.119110	35.195584
1148.258683	116987.495410	35.200602
1149.328093	117206.720654	35.205620
1150.826479	117417.843484	35.210637
1151.974700	117628.594948	35.215655
1152.828359	117839.383978	35.220672
1154.199858	118048.200981	35.225690
1155.600548	118257.268089	35.230708
1156.671905	118466.885324	35.235725
1157.434140	118677.720924	35.240743
1159.041340	118868.157032	35.245760
1160.083605	119090.112713	35.250778
1161.035654	119287.375689	35.255796
1162.759197	119499.908369	35.260813
1163.682739	119715.349931	35.265831
1164.713331	119910.982171	35.270848
1165.918905	120110.527720	35.275866
1167.267504	120313.535753	35.280884
1168.502177	120507.389520	35.285901
1169.300587	120693.612078	35.290919
1170.926731	120902.812949	35.295936
1171.648566	121079.470473	35.300954
1172.734697	121273.708661	35.305972
1174.149280	121476.523720	35.310989
1175.027684	121673.624814	35.316007
1176.289339	121873.249064	35.321024
1177.215814	122072.663939	35.326042
1178.245975	122272.227756	35.331060
1179.751630	122479.926288	35.336077
1180.374548	122678.102769	35.341095
1181.963021	122895.523287	35.346112
1182.802789	123106.289055	35.351130
1184.125542	123318.433879	35.356148
1185.520836	123524.713171	35.361165
1186.407715	123750.822985	35.366183
1187.329517	123957.259552	35.371200
1188.647781	124165.190839	35.376218
1189.553877	124389.908181	35.381236
1191.100606	124621.200338	35.386253
1192.246985	124847.997869	35.391271
1193.291564	125065.055022	35.396288
1194.639249	125294.877022	35.401306
1195.771938	125521.187552	35.406324
1197.029678	125742.029192	35.411341
1198.375763	125966.381272	35.416359
1199.593602	126189.514108	35.421376
1200.886239	126415.652724	35.426394
1201.802386	126643.325485	35.431412
1203.407031	126867.501993	35.436429
1204.489816	127105.708604	35.441447
1205.705579	127323.235095	35.446464
1207.437724	127551.058518	35.451482
1208.235328	127774.006114	35.456500
1209.758069	128010.233033	35.461517
1211.146184	128240.285826	35.466535
1212.588859	128450.393069	35.471552
1213.772088	128676.211375	35.476570
1215.120435	128900.102699	35.481588
1216.691456	129103.830036	35.486605
1217.577594	129325.747363	35.491623
1218.293473	129550.254897	35.496640
1219.918977	129768.630689	35.501658
1220.921484	129994.184128	35.506676
1222.393970	130213.222087	35.511693
1223.409801	130447.117362	35.516711
1224.843475	130662.133845	35.521728
1225.700352	130890.329030	35.526746
1226.915628	131125.083671	35.531764
1228.185536	131338.902192	35.536781
1229.248175	131565.851264	35.541799
1230.436357	131793.047404	35.546816
1232.012697	132023.489619	35.551834
1233.015544	132255.004397	35.556852
1234.898313	132493.246279	35.561869
1235.356194	132722.750133	35.566887
1236.822412	132947.651970	35.571904
1238.263401	133173.142693	35.576922
1239.320017	133409.093870	35.581940
1240.684325	133632.610134	35.586957
1241.720442	133864.878902	35.591975
1242.638619	134094.785444	35.596992
1244.044603	134336.225675	35.602010
1244.966571	134564.588227	35.607028
1246.802236	134798.709201	35.612045
1247.852004	135040.074042	35.617063
1249.288575	135264.717853	35.622080
1250.338936	135491.480878	35.627098
1251.274201	135715.018878	35.632116
1252.890545	135932.487044	35.637133
1254.190147	136149.844174	35.642151
1255.503822	136373.197286	35.647168
1256.535951	136584.693336	35.652186
1257.709773	136819.457838	35.657204
1259.268656	137036.080582	35.662221
1260.152068	137266.801024	35.667239
1261.220287	137488.072140	35.672256
1262.651414	137726.464658	35.677274
1263.266342	137965.526289	35.682292
1264.970844	138192.250276	35.687309
1266.361642	138435.827550	35.692327
1267.687732	138671.137708	35.697344
1269.001612	138898.463525	35.702362
1270.312920	139132.917135	35.707380
1271.788483	139374.230197	35.712397
1272.642539	139614.937632	35.717415
1273.804078	139850.524058	35.722432
1275.222270	140093.525406	35.727450
1276.540405	140345.509695	35.732468
1277.950612	140577.598404	35.737485
1279.120618	140823.714490	35.742503
1279.989751	141071.847482	35.747520
1281.819355	141324.324997	35.752538
1283.091721	141585.430322	35.757556
1284.490332	141813.661738	35.762573
1286.176930	142069.249650	35.767591
1286.940931	142310.320452	35.772608
1288.531326	142555.491684	35.777626
1289.457337	142805.326842	35.782644
1291.010662	143049.518554	35.787661
1292.277323	143302.686739	35.792679
1293.523679	143544.307656	35.797696
1294.907441	143798.322354	35.802714
1296.088231	144060.120655	35.807732
1297.625531	144314.722376	35.812749
1298.552574	144566.624186	35.817767
1299.878364	144821.074262	35.822784
1301.177320	145078.929253	35.827802
1302.618534	145340.072511	35.832820
1303.908883	145587.711141	35.837837
1305.415001	145839.881287	35.842855
1306.652817	146099.757443	35.847872
1308.266617	146356.707184	35.852890
1309.413816	146629.487084	35.857908
1310.678487	146870.899134	35.862925
1312.399369	147133.404173	35.867943
1313.565873	147384.537827	35.872960
1315.044917	147631.689978	35.877978
1316.093958	147893.575927	35.882996
1317.504736	148144.344667	35.888013
1318.972141	148409.272398	35.893031
1320.125906	148663.080276	35.898048
1321.721590	148907.215879	35.903066
1322.444072	149178.727845	35.908084
1324.143157	149416.787226	35.913101
1325.755314	149685.276787	35.918119
1327.101217	149937.996227	35.923136
1328.347667	150189.338640	35.928154
1329.164575	150438.508754	35.933172
1330.683076	150692.561881	35.938189
1332.025208	150955.004376	35.943207
1333.215817	151202.481590	35.948224
1334.712367	151458.446051	35.953242
1336.044217	151726.882344	35.958260
1337.598546	151974.887941	35.963277
1338.830972	152213.993414	35.968295
1340.132172	152460.433125	35.973312
1341.416560	152685.922894	35.978330
1342.626547	152934.410196	35.983348
1343.604596	153181.808523	35.988365
1345.231403	153427.185868	35.993383
1346.448476	153684.391041	35.998400
1347.503298	153918.678277	36.003418
1348.750048	154177.632288	36.008436
1349.865716	154438.512398	36.013453
1351.431989	154691.987935	36.018471
1352.833512	154956.020840	36.023488
1354.511197	155211.409436	36.028506
1355.644364	155474.411945	36.033524
1356.795920	155739.899466	36.038541
1358.226655	156009.693681	36.043559
1359.247984	156277.946349	36.048576
1360.848338	156535.423988	36.053594
1362.129063	156808.813026	36.058612
1363.629254	157086.835973	36.063629
1365.069119	157358.971964	36.068647
1366.457008	157632.615311	36.073664
1367.848663	157910.699951	36.078682
1368.848933	158192.847263	36.083700
1370.365139	158461.781210	36.088717
1371.705541	158746.540232	36.093735
1372.992139	159031.513116	36.098752
1374.564994	159307.902788	36.103770
1375.983621	159594.545052	36.108788
1377.183821	159884.752256	36.113805
1378.898639	160157.559277	36.118823
1380.023212	160453.453876	36.123840
1381.441799	160740.040666	36.128858
1382.741971	161031.305070	36.133876
1384.545068	161312.706773	36.138893
1386.132640	161605.488179	36.143911
1387.426876	161879.530503	36.148928
1389.099709	162164.296153	36.153946
1390.253435	162445.482888	36.158964
1391.754768	162728.212653	36.163981
1393.249052	163011.440277	36.168999
1394.487666	163294.750097	36.174016
1396.189533	163586.041873	36.179034
1397.730914	163872.046008	36.184052
1398.753459	164156.869005	36.189069
1400.414523	164434.267473	36.194087
1401.499170	164731.606919	36.199104
1403.041243	165014.078568	36.204122
1404.504147	165304.761654	36.209140
1406.308476	165586.876477	36.214157
1407.375560	165870.789801	36.219175
1408.538866	166166.590741	36.224192
1410.261832	166452.010855	36.229210
1411.456316	166743.534506	36.234228
1412.915487	167029.636363	36.239245
1414.574307	167323.180710	36.244263
1415.547071	167610.635546	36.249280
1417.274710	167890.709462	36.254298
1418.815508	168192.412571	36.259316
1420.172403	168467.031654	36.264333
1421.759228	168757.526537	36.269351
1423.034551	169051.640416	36.274368
1424.655308	169338.440858	36.279386
1425.798268	169620.474730	36.284404
1427.287351	169901.996326	36.289421
1428.924551	170199.648900	36.294439
1430.208529	170487.260862	36.299456
1431.627379	170760.906397	36.304474
1433.246856	171035.484814	36.309492
1434.665197	171304.882582	36.314509
1436.098957	171571.601794	36.319527
1437.325299	171843.331259	36.324544
1438.771426	172110.165702	36.329562
1440.045431	172376.002201	36.334580
1441.211283	172655.944149	36.339597
1443.116926	172931.006667	36.344615
1443.842583	173219.044904	36.349632
1445.450689	173501.532956	36.354650
1447.098764	173790.018662	36.359668
1448.137760	174077.616882	36.364685
1450.022128	174362.297885	36.369703
1450.654775	174656.527747	36.374720
1452.243005	174956.502701	36.379738
1453.967183	175254.464576	36.384756
1455.434082	175550.465614	36.389773
1456.723932	175845.710851	36.394791
1458.411867	176161.641997	36.399808
1459.653243	176452.380850	36.404826
1461.221080	176762.599274	36.409844
1462.730752	177075.481727	36.414861
1464.131810	177356.757138	36.419879
1465.659299	177669.386532	36.424896
1467.467510	177971.539034	36.429914
1468.684747	178283.817371	36.434932
1469.907333	178598.622395	36.439949
1471.839037	178906.534785	36.444967
1473.036401	179220.637074	36.449984
1474.785871	179522.351579	36.455002
1476.371157	179848.463629	36.460020
1477.717388	180173.652636	36.465037
1479.360624	180470.072239	36.470055
1480.812196	180792.430046	36.475072
1482.330749	181103.431841	36.480090
1483.425496	181408.819312	36.485108
1485.300940	181736.545213	36.490125
1486.332323	182041.553340	36.495143
1487.795440	182367.117373	36.500160
1489.633341	182684.701225	36.505178
1491.298765	183019.247606	36.510196
1492.602761	183340.693300	36.515213
1494.191369	183657.372110	36.520231
1495.594201	184000.852987	36.525248
1497.133191	184321.707159	36.530266
1499.236967	184651.672423	36.535284
1500.297524	184966.605549	36.540301
1501.808249	185291.316083	36.545319
1502.987161	185610.371322	36.550336
1505.041528	185922.873550	36.555354
1506.728404	186249.883454	36.560372
1507.992902	186576.381139	36.565389
1509.974959	186891.617119	36.570407
1511.162178	187208.649052	36.575424
1512.773135	187533.406726	36.580442
1514.102534	187853.147904	36.585460
1515.708286	188177.719670	36.590477
1517.540618	188490.006101	36.595495
1518.731307	188804.012371	36.600512
1520.172116	189128.578616	36.605530
1521.806929	189449.522139	36.610548
1523.266180	189779.979049	36.615565
1525.187794	190103.455681	36.620583
1526.405039	190427.278947	36.625600
1528.191514	190747.937851	36.630618
1529.929418	191066.042190	36.635636
1531.117342	191379.897512	36.640653
1532.520833	191691.256071	36.645671
1534.305317	192008.710232	36.650688
1535.577823	192289.232535	36.655706
1537.231937	192601.392176	36.660724
1538.383379	192899.545059	36.665741
1539.992156	193189.219725	36.670759
1541.760149	193513.057235	36.675776
1543.158608	193812.430484	36.680794
1544.571781	194125.170760	36.685812
1546.101044	194440.254719	36.690829
1547.880017	194736.789219	36.695847
1548.948527	195062.400621	36.700864
1550.372696	195368.784803	36.705882
1552.059027	195682.312780	36.710900
1553.332681	196008.504449	36.715917
1554.864673	196331.646208	36.720935
1556.045572	196668.863605	36.725952
1557.467951	196995.187966	36.730970
1559.169752	197332.068776	36.735988
1560.371615	197676.702200	36.741005
1562.084824	198023.487404	36.746023
1563.568222	198365.830671	36.751040
1565.113043	198710.234981	36.756058
1566.896821	199064.276015	36.761076
1568.473599	199418.149938	36.766093
1569.949028	199779.228512	36.771111
1571.666959	200138.567595	36.776128
1573.031891	200491.466288	36.781146
1574.987668	200841.514011	36.786164
1576.471109	201193.698341	36.791181
1578.401456	201539.982850	36.796199
1579.802412	201909.654857	36.801216
1581.205990	202259.686505	36.806234
1583.233156	202623.608676	36.811252
1584.198925	202982.705458	36.816269
1586.343592	203334.689425	36.821287
1587.917125	203696.711150	36.826304
1589.292529	204064.569912	36.831322
1591.233076	204423.868161	36.836340
1592.862193	204785.225725	36.841357
1594.803402	205142.025944	36.846375
1596.110987	205509.153810	36.851392
1597.697813	205857.559529	36.856410
1599.716004	206222.719591	36.861428
1601.029754	206574.805095	36.866445
1602.615410	206934.745108	36.871463
1604.664353	207294.521343	36.876480
1606.038674	207660.111886	36.881498
1607.565494	208021.958486	36.886516
1609.550452	208390.600498	36.891533
1611.203095	208742.271347	36.896551
1612.587948	209104.539855	36.901568
1613.962316	209462.354724	36.906586
1615.931430	209813.647721	36.911604
1617.288105	210190.172724	36.916621
1619.011475	210545.407669	36.921639
1620.498028	210913.051188	36.926656
1622.486079	211269.997771	36.931674
1624.197428	211627.524868	36.936692
1625.317767	212004.985777	36.941709
1627.288378	212360.949261	36.946727
1628.839065	212726.837493	36.951744
1630.312278	213096.905116	36.956762
1631.975813	213456.250702	36.961780
1633.612887	213831.830817	36.966797
1635.134155	214188.409127	36.971815
1637.114189	214551.211559	36.976832
1638.441198	214925.171146	36.981850
1640.427416	215289.499280	36.986868
1641.727383	215637.687744	36.991885
1643.447590	215981.084101	36.996903
1644.521242	216334.696799	37.001920
1646.253000	216679.973178	37.006938
1648.164341	217025.652882	37.011956
1649.631093	217395.611562	37.016973
1651.006348	217740.391807	37.021991
1652.792402	218109.132084	37.027008
1654.241933	218462.842712	37.032026
1655.772806	218828.960944	37.037044
1656.938693	219206.773278	37.042061
1658.732167	219565.586783	37.047079
1660.127034	219949.434246	37.052096
1661.467459	220330.523634	37.057114
1663.855290	220718.781632	37.062132
1665.153673	221112.453173	37.067149
1666.648812	221495.603839	37.072167
1668.281384	221894.658383	37.077184
1669.856718	222293.546019	37.082202
1671.488199	222684.577415	37.087220
1672.941179	223103.807560	37.092237
1674.704543	223499.696642	37.097255
1676.449814	223914.487337	37.102272
1678.258451	224315.731013	37.107290
1679.415959	224804.382519	37.112308
1681.392873	225221.806475	37.117325
1683.297397	225643.384003	37.122343
1684.586925	226070.017555	37.127360
1686.436707	226473.395126	37.132378
1688.138836	226902.096945	37.137396
1689.814445	227336.824435	37.142413
1691.812754	227748.614357	37.147431
1693.427629	228182.465666	37.152448
1695.072013	228599.726973	37.157466
1696.924197	229028.182293	37.162484
1698.669956	229456.732727	37.167501
1700.609049	229878.521341	37.172519
1702.205929	230308.216586	37.177536
1704.012262	230740.139194	37.182554
1706.034441	231165.600979	37.187572
1707.543154	231595.619377	37.192589
1709.491392	232020.968799	37.197607
1711.023241	232448.115458	37.202624
1712.511828	232879.842656	37.207642
1714.837816	233309.883232	37.212660
1716.537448	233739.393378	37.217677
1718.065779	234169.898198	37.222695
1720.146712	234591.574732	37.227712
1721.574844	235018.288044	37.232730
1723.761608	235450.871890	37.237748
1725.600135	235880.796336	37.242765
1727.150892	236294.131190	37.247783
1729.052270	236714.089744	37.252800
1730.427784	237141.528046	37.257818
1732.749590	237565.000721	37.262836
1734.413467	237994.704870	37.267853
1735.785881	238418.387004	37.272871
1737.821640	238836.194189	37.277888
1739.236039	239269.676362	37.282906
1741.432382	239687.306315	37.287924
1742.539176	240119.215280	37.292941
1744.583496	240543.552772	37.297959
1746.342171	240956.430982	37.302976
1747.746619	241404.906371	37.307994
1749.618730	241833.974115	37.313012
1751.561561	242259.550797	37.318029
1753.552606	242694.646186	37.323047
1755.019187	243109.252862	37.328064
1756.704405	243526.440549	37.333082
1758.550278	243925.261641	37.338100
1760.204148	244339.382024	37.343117
1762.027420	244737.674543	37.348135
1763.640856	245147.687521	37.353152
1765.267907	245553.253319	37.358170
1767.232046	245965.394102	37.363188
1768.898962	246380.531232	37.368205
1770.587958	246794.852340	37.373223
1772.163122	247209.370566	37.378240
1773.749408	247634.861502	37.383258
1775.378801	248043.808479	37.388276
1777.190477	248490.245994	37.393293
1779.096998	248922.264830	37.398311
1780.743102	249353.082372	37.403328
1782.230551	249793.020834	37.408346
1784.411726	250232.845141	37.413364
1785.894295	250679.212213	37.418381
1787.661450	251119.715354	37.423399
1789.701771	251570.258788	37.428416
1791.184032	252008.320170	37.433434
1793.002513	252465.835982	37.438452
1794.681182	252918.777221	37.443469
1796.657455	253373.676451	37.448487
1798.536143	253823.638433	37.453504
1799.910541	254289.967420	37.458522
1802.023097	254745.581569	37.463540
1803.797286	255219.821588	37.468557
1805.674408	255679.818959	37.473575
1807.573998	256137.221637	37.478592
1809.397313	256611.174584	37.483610
1811.465959	257077.770974	37.488628
1813.145203	257551.062019	37.493645
1814.989941	258009.795102	37.498663
1816.720973	258481.909134	37.503680
1818.331627	258959.962024	37.508698
1820.431353	259438.442192	37.513716
1822.268746	259919.836212	37.518733
1823.964973	260380.194139	37.523751
1825.931239	260848.738045	37.528768
1827.435648	261345.047684	37.533786
1829.652661	261819.468870	37.538804
1831.644193	262304.215439	37.543821
1833.158905	262791.784092	37.548839
1835.142041	263262.813847	37.553856
1837.139379	263766.611163	37.558874
1839.252017	264237.085515	37.563892
1841.071678	264718.734543	37.568909
1843.334227	265197.312511	37.573927
1845.431819	265682.141125	37.578944
1846.886732	266148.073926	37.583962
1848.787788	266625.059210	37.588980
1850.870287	267100.439095	37.593997
1852.567666	267564.272913	37.599015
1854.738259	268043.092110	37.604032
1856.371105	268510.949277	37.609050
1858.308497	268993.717972	37.614068
1859.720039	269471.695550	37.619085
1861.827367	269949.608426	37.624103
1864.086455	270424.548874	37.629120
1865.582150	270893.899097	37.634138
1867.455716	271373.652212	37.639156
1869.419062	271858.851377	37.644173
1871.143901	272345.562523	37.649191
1873.281678	272807.513278	37.654208
1874.964256	273303.552593	37.659226
1876.812389	273765.524214	37.664244
1878.478213	274242.919092	37.669261
1880.536235	274698.503794	37.674279
1882.481550	275148.060506	37.679296
1884.018280	275603.602633	37.684314
1885.936447	276059.055507	37.689332
1887.751722	276523.872537	37.694349
1889.536328	276985.772425	37.699367
1891.508456	277435.167906	37.704384
1893.466679	277906.359798	37.709402
1895.126880	278370.334857	37.714420
1897.149110	278841.336261	37.719437
1898.920054	279325.129852	37.724455
1901.024200	279795.505832	37.729472
1902.302883	280271.935603	37.734490
1904.291859	280740.346926	37.739508
1906.342467	281232.700705	37.744525
1907.964803	281717.681179	37.749543
1910.150731	282194.133935	37.754560
1911.983710	282693.657426	37.759578
1913.976078	283186.370947	37.764596
1915.677119	283685.456050	37.769613
1917.477360	284179.620799	37.774631
1919.404105	284675.160197	37.779648
1921.167664	285192.925547	37.784666
1923.292746	285694.550608	37.789684
1925.404820	286209.562444	37.794701
1927.169661	286719.981470	37.799719
1929.384188	287225.295100	37.804736
1931.002533	287744.370945	37.809754
1933.200868	288256.084536	37.814772
1935.079229	288767.849062	37.819789
1936.740191	289281.374778	37.824807
1938.728247	289806.858839	37.829824
1940.995464	290333.513905	37.834842
1942.888418	290854.665999	37.839860
1945.065512	291381.712626	37.844877
1946.875057	291902.543948	37.849895
1949.083741	292416.906417	37.854912
1950.894139	292945.480063	37.859930
1952.952235	293476.906007	37.864948
1955.037873	293999.638395	37.869965
1957.188964	294526.853284	37.874983
1958.993688	295043.582260	37.880000
1961.178379	295572.894850	37.885018
1963.115762	296092.416349	37.890036
1965.074289	296613.862191	37.895053
1967.150198	297142.702541	37.900071
1969.309398	297672.237660	37.905088
1971.229997	298201.555509	37.910106
1973.497469	298719.841302	37.915124
1975.477756	299237.867097	37.920141
1976.979313	299771.563664	37.925159
1979.049773	300289.696106	37.930176
1981.332866	300814.800485	37.935194
1983.230895	301343.241887	37.940212
1985.454943	301862.839007	37.945229
1987.315689	302402.760336	37.950247
1989.522341	302914.608314	37.955264
1991.362641	303432.913998	37.960282
1993.307678	303956.862953	37.965300
1995.611282	304488.800433	37.970317
1997.206216	305009.651833	37.975335
1999.159085	305535.901294	37.980352
2001.230075	306053.417136	37.985370
2003.330823	306588.016566	37.990388
2005.436475	307110.193187	37.995405
2006.999636	307646.246077	38.000423
2009.230163	308168.268504	38.005440
2011.152646	308686.275200	38.010458
2013.086702	309196.150182	38.015476
2015.035163	309687.709630	38.020493
2016.862450	310201.328954	38.025511
2019.136606	310703.037157	38.030528
2021.201673	311204.446537	38.035546
2023.241739	311713.805299	38.040564
2024.997749	312215.436905	38.045581
2026.773445	312739.485040	38.050599
2029.078433	313247.901005	38.055616
2030.947531	313773.424750	38.060634
2032.463167	314280.999006	38.065652
2034.535773	314822.936764	38.070669
2036.787205	315353.540937	38.075687
2038.778446	315893.935107	38.080704
2040.418375	316427.019234	38.085722
2042.535081	316959.944446	38.090740
2044.664727	317506.803959	38.095757
2046.499503	318054.114115	38.100775
2048.521466	318599.103716	38.105792
2050.238508	319154.753113	38.110810
2052.513537	319709.112402	38.115828
2054.588711	320288.866180	38.120845
2056.552625	320846.771370	38.125863
2058.617083	321409.200214	38.130880
2060.803917	321980.287650	38.135898
2062.848587	322541.643501	38.140916
2065.005434	323119.606593	38.145933
2067.184263	323693.777646	38.150951
2069.290662	324257.317026	38.155968
2071.043918	324844.877452	38.160986
2073.191571	325418.809209	38.166004
2075.406708	326000.645861	38.171021
2076.987858	326592.813330	38.176039
2079.598627	327174.167120	38.181056
2081.615600	327774.933862	38.186074
2083.933815	328357.644535	38.191092
2086.154951	328951.967714	38.196109
2087.927760	329546.815794	38.201127
2090.247553	330142.151334	38.206144
2092.341492	330719.950046	38.211162
2094.444886	331321.173384	38.216180
2096.547445	331910.230236	38.221197
2098.679062	332518.036556	38.226215
2100.871393	333099.780072	38.231232
2102.509902	333708.213132	38.236250
2104.966783	334310.081753	38.241268
2107.458838	334901.352212	38.246285
2109.287490	335513.998214	38.251303
2111.433542	336112.191661	38.256320
2113.757177	336721.289644	38.261338
2115.478005	337321.189473	38.266356
2117.751626	337924.544830	38.271373
2119.836292	338536.503906	38.276391
2121.904381	339144.320928	38.281408
2123.792813	339765.613215	38.286426
2125.558624	340374.429864	38.291444
2128.165312	340992.187107	38.296461
2129.966612	341610.627990	38.301479
2132.179028	342229.170897	38.306496
2134.402835	342851.181309	38.311514
2136.558803	343478.245729	38.316532
2139.011678	344085.582999	38.321549
2140.921229	344717.164234	38.326567
2143.184285	345328.780834	38.331584
2145.479817	345952.058730	38.336602
2147.437604	346577.160602	38.341620
2149.691480	347189.287306	38.346637
2151.862356	347799.389283	38.351655
2154.211010	348399.175585	38.356672
2157.003027	348975.761502	38.361690
2158.756701	349564.565799	38.366708
2160.786536	350144.282475	38.371725
2162.591713	350731.692518	38.376743
2164.811251	351320.472832	38.381760
2167.105632	351913.826007	38.386778
2169.045283	352501.393219	38.391796
2171.303065	353097.324650	38.396813
2173.329319	353696.001209	38.401831
2175.580186	354288.060248	38.406848
2177.715354	354891.269554	38.411866
2179.768664	355502.248254	38.416884
2182.090980	356096.629992	38.421901
2183.930115	356705.165263	38.426919
2186.467698	357313.068874	38.431936
2188.720283	357934.356579	38.436954
2190.396709	358556.440398	38.441972
2192.818349	359166.847526	38.446989
2194.983394	359801.542937	38.452007
2197.286757	360426.488395	38.457024
2199.456230	361053.856404	38.462042
2201.600128	361680.203928	38.467060
2204.105265	362304.883599	38.472077
2206.396508	362948.590363	38.477095
2208.815762	363570.473380	38.482112
2211.200102	364205.493147	38.487130
2213.031017	364839.705916	38.492148
2215.359866	365468.270464	38.497165
2217.532766	366114.886585	38.502183
2219.467313	366751.054467	38.507200
2222.088458	367398.081974	38.512218
2224.181374	368054.393360	38.517236
2226.682234	368688.202638	38.522253
2229.008894	369348.637875	38.527271
2230.984203	369989.233303	38.532288
2233.528103	370625.969748	38.537306
2235.664638	371286.198448	38.542324
2238.182662	371925.427348	38.547341
2240.492510	372585.781172	38.552359
2242.817586	373223.446254	38.557376
2245.414442	373873.203422	38.562394
2247.249488	374510.697948	38.567412
2249.860458	375163.117307	38.572429
2251.896803	375817.648162	38.577447
2254.197441	376462.334063	38.582464
2256.441108	377113.154361	38.587482
2258.572563	377776.711132	38.592500
2261.083273	378426.853771	38.597517
2263.065783	379082.726008	38.602535
2265.156241	379733.242586	38.607552
2267.914443	380387.287796	38.612570
2269.864115	381056.946566	38.617588
2272.696800	381710.699935	38.622605
2274.650238	382361.263889	38.627623
2276.594881	383020.107559	38.632640
2279.200221	383673.098765	38.637658
2281.089794	384339.835512	38.642676
2283.668244	385001.450170	38.647693
2285.938414	385663.786636	38.652711
2288.231307	386336.043849	38.657728
2290.537826	386993.859322	38.662746
2292.750070	387662.501781	38.667764
2295.498964	388320.495490	38.672781
2297.736351	388986.164929	38.677799
2300.275951	389645.686315	38.682816
2302.544343	390301.765581	38.687834
2304.897617	390955.636899	38.692852
2306.918849	391576.723075	38.697869
2309.157406	392197.177771	38.702887
2311.524778	392832.452049	38.707904
2314.165628	393452.611916	38.712922
2316.160733	394076.794251	38.717940
2318.534067	394704.753726	38.722957
2320.626294	395342.757714	38.727975
2323.099407	395966.872350	38.732992
2325.541995	396597.365560	38.738010
2327.506923	397229.368678	38.743028
2329.938845	397869.593596	38.748045
2331.908301	398514.239676	38.753063
2333.981576	399161.793969	38.758080
2336.323262	399815.295341	38.763098
2338.589972	400475.813609	38.768116
2341.017667	401131.475459	38.773133
2343.301477	401794.342389	38.778151
2345.308251	402469.427560	38.783168
2347.458335	403139.430624	38.788186
2350.029666	403821.814340	38.793204
2352.380086	404506.168815	38.798221
2354.726348	405188.961629	38.803239
2357.009969	405876.891122	38.808256
2359.519886	406563.245999	38.813274
2361.697478	407264.129901	38.818292
2364.101020	407952.164927	38.823309
2366.486465	408654.017472	38.828327
2368.497008	409361.132186	38.833344
2371.389064	410067.322914	38.838362
2373.688923	410780.736160	38.843380
2376.126069	411490.156107	38.848397
2378.401091	412204.852464	38.853415
2380.584452	412912.756397	38.858432
2383.129378	413634.968200	38.863450
2385.540376	414370.276640	38.868468
2388.052659	415078.599609	38.873485
2390.752910	415798.775615	38.878503
2393.372046	416529.024526	38.883520
2395.947223	417238.037623	38.888538
2398.170033	417970.564785	38.893556
2400.788260	418689.710777	38.898573
2402.746794	419408.894569	38.903591
2405.597521	420126.948400	38.908608
2408.277173	420851.441545	38.913626
2410.425085	421580.964272	38.918644
2413.275774	422300.044463	38.923661
2415.927894	423014.224630	38.928679
2418.176477	423732.805467	38.933696
2421.158347	424450.586019	38.938714
2423.294591	425171.573687	38.943732
2425.553152	425883.152836	38.948749
2428.100235	426603.220097	38.953767
2430.846727	427311.486959	38.958784
2433.087816	428039.054906	38.963802
2435.874597	428752.284698	38.968820
2438.375927	429460.579001	38.973837
2440.695853	430172.121972	38.978855
2443.447363	430885.951517	38.983872
2445.799286	431591.219890	38.988890
2447.987918	432308.844924	38.993908
2450.520863	433020.873803	38.998925
2453.237933	433723.587822	39.003943
2455.479568	434434.558409	39.008960
2458.402194	435147.520414	39.013978
2460.640993	435859.358425	39.018996
2463.410336	436560.205719	39.024013
2465.865492	437262.196633	39.029031
2468.100786	437963.999656	39.034048
2470.425037	438632.873159	39.039066
2472.477399	439312.398293	39.044084
2475.396186	439981.386528	39.049101
2478.009880	440652.277247	39.054119
2480.157377	441332.686573	39.059136
2482.627162	441990.961515	39.064154
2484.974486	442678.177663	39.069172
2487.433376	443356.651768	39.074189
2490.175701	444038.548962	39.079207
2492.541969	444716.034901	39.084224
2494.958667	445397.133827	39.089242
2497.303362	446090.920695	39.094260
2499.386534	446787.358871	39.099277
2501.880967	447483.757217	39.104295
2504.585422	448196.436449	39.109312
2506.911720	448890.186411	39.114330
2509.146567	449620.092984	39.119348
2511.517141	450329.923313	39.124365
2514.119717	451044.597328	39.129383
2516.151252	451781.796121	39.134400
2518.706911	452511.195497	39.139418
2520.982965	453254.572932	39.144436
2523.297039	453999.333408	39.149453
2526.118998	454754.147205	39.154471
2528.345831	455520.004120	39.159488
2530.989490	456264.881154	39.164506
2533.477904	457028.110373	39.169524
2536.332314	457797.216597	39.174541
2538.730725	458570.514586	39.179559
2541.091437	459349.350289	39.184576
2543.984648	460119.170595	39.189594
2546.605461	460900.582560	39.194612
2549.077356	461677.135755	39.199629
2551.678898	462458.590896	39.204647
2554.064964	463235.956568	39.209664
2556.762292	464029.009840	39.214682
2559.133897	464816.929618	39.219700
2561.773908	465613.264026	39.224717
2564.699119	466415.583341	39.229735
2567.092866	467215.026142	39.234752
2569.563014	468014.726505	39.239770
2572.274644	468813.949596	39.244788
2574.705386	469617.632293	39.249805
2577.250599	470413.935939	39.254823
2579.843239	471229.145222	39.259840
2582.722873	472029.367995	39.264858
2585.403579	472839.895851	39.269876
2588.125035	473653.059548	39.274893
2590.767716	474462.412279	39.279911
2593.447244	475273.188764	39.284928
2596.230301	476073.760013	39.289946
2598.425556	476879.394085	39.294964
2601.230554	477694.337275	39.299981
2604.000151	478495.462349	39.304999
2606.703943	479306.158781	39.310016
2609.475243	480107.465487	39.315034
2612.405386	480914.719986	39.320052
2615.099290	481719.755667	39.325069
2617.716337	482518.052460	39.330087
2620.365868	483314.995687	39.335104
2623.091262	484117.596255	39.340122
2625.742431	484911.893122	39.345140
2628.150933	485709.778979	39.350157
2630.965021	486501.352678	39.355175
2633.513630	487307.422522	39.360192
2636.382058	488098.966013	39.365210
2638.878629	488902.548319	39.370228
2641.380328	489688.225274	39.375245
2644.130269	490449.902534	39.380263
2646.683252	491210.519004	39.385280
2649.332678	491969.925383	39.390298
2651.696903	492726.670734	39.395316
2654.199842	493495.117578	39.400333
2656.912804	494252.293178	39.405351
2659.726112	495029.097141	39.410368
2662.445142	495791.501383	39.415386
2664.796283	496568.260708	39.420404
2667.116899	497347.259644	39.425421
2669.818057	498125.302150	39.430439
2672.261565	498914.953682	39.435456
2675.312040	499696.195048	39.440474
2677.704381	500493.195600	39.445492
2679.886780	501299.977684	39.450509
2682.567665	502108.151326	39.455527
2684.907203	502915.837343	39.460544
2687.629364	503740.869841	39.465562
2690.497860	504569.366674	39.470580
2693.185367	505402.994795	39.475597
2695.725982	506220.872245	39.480615
2698.136246	507062.427870	39.485632
2700.970254	507907.701579	39.490650
2703.401536	508745.434966	39.495668
2705.895837	509604.287746	39.500685
2709.152487	510460.347313	39.505703
2711.731549	511331.947792	39.510720
2715.016528	512179.492057	39.515738
2717.406186	513054.103760	39.520756
2720.257901	513908.985369	39.525773
2723.189424	514772.223534	39.530791
2725.835091	515644.632924	39.535808
2728.666876	516517.013218	39.540826
2731.403896	517384.422138	39.545844
2734.132457	518261.004402	39.550861
2736.842739	519134.567336	39.555879
2739.566590	520018.456622	39.560896
2742.445404	520897.836233	39.565914
2745.499924	521780.360159	39.570932
2748.086736	522662.859680	39.575949
2751.299826	523541.527710	39.580967
2753.547290	524434.809032	39.585984
2756.851461	525315.423699	39.591002
2759.705591	526197.420616	39.596020
2762.864487	527076.898175	39.601037
2765.905074	527947.179089	39.606055
2768.445954	528840.048309	39.611072
2771.394462	529717.239212	39.616090
2774.256292	530597.765324	39.621108
2776.899194	531477.368686	39.626125
2779.608679	532356.052539	39.631143
2782.018002	533238.508176	39.636160
2785.228233	534109.906536	39.641178
2788.302305	534991.995092	39.646196
2790.816269	535886.250754	39.651213
2793.662136	536760.619366	39.656231
2796.455010	537645.963520	39.661248
2799.223131	538529.495939	39.666266
2802.491794	539399.407104	39.671284
2804.954275	540286.453244	39.676301
2807.920136	541169.537535	39.681319
2810.256268	542058.103337	39.686336
2813.182449	542940.831791	39.691354
2816.248634	543831.126912	39.696372
2818.837756	544710.932513	39.701389
2821.903310	545596.538439	39.706407
2824.767418	546490.167279	39.711424
2827.358951	547361.708377	39.716442
2830.181320	548210.730743	39.721460
2832.849735	549065.860167	39.726477
2835.750718	549911.596995	39.731495
2838.251865	550753.174885	39.736512
2840.609197	551599.098039	39.741530
2843.710720	552459.825228	39.746548
2846.057833	553327.055869	39.751565
2849.018896	554194.933812	39.756583
2851.666551	555068.788088	39.761600
2854.346402	555952.178604	39.766618
2857.073214	556822.739649	39.771636
2859.980309	557721.000598	39.776653
2863.044150	558624.400383	39.781671
2865.179184	559526.987517	39.786688
2867.787057	560429.485352	39.791706
2870.830865	561345.663574	39.796724
2873.289470	562269.258148	39.801741
2876.056199	563189.120572	39.806759
2879.104665	564130.165959	39.811776
2882.081498	565057.997889	39.816794
2885.466021	566001.011807	39.821812
2888.223127	566942.001773	39.826829
2891.271100	567891.510809	39.831847
2894.038612	568838.987792	39.836864
2896.927956	569778.342600	39.841882
2900.067775	570731.140043	39.846900
2902.566396	571700.585643	39.851917
2905.689538	572650.130021	39.856935
2908.578917	573626.490609	39.861952
2911.624633	574586.290413	39.866970
2914.727358	575562.867046	39.871988
2917.755905	576536.720577	39.877005
2920.623093	577500.039344	39.882023
2924.085301	578468.803963	39.887040
2927.088870	579447.550681	39.892058
2929.667118	580416.760112	39.897076
2932.920407	581401.831182	39.902093
2935.824457	582365.466962	39.907111
2938.825522	583356.039414	39.912128
2941.997853	584328.903557	39.917146
2945.185788	585291.709955	39.922164
2948.074235	586282.313430	39.927181
2951.204041	587267.833137	39.932199
2954.018821	588247.860534	39.937216
2956.957240	589220.670384	39.942234
2960.348786	590197.736813	39.947252
2963.067959	591189.968267	39.952269
2966.405034	592154.505343	39.957287
2969.787478	593130.781253	39.962304
2972.678656	594115.624776	39.967322
2975.973051	595076.022754	39.972340
2978.746539	596045.544959	39.977357
2982.064333	597009.838293	39.982375
2984.997232	597986.586430	39.987392
2987.786153	598956.715923	39.992410
2991.263205	599923.746517	39.997428
2994.094176	600895.309274	40.002445
2996.650086	601857.673273	40.007463
2999.871530	602825.404072	40.012480
3002.877142	603803.801415	40.017498
3005.801192	604767.862942	40.022516
3008.575234	605735.871725	40.027533
3011.640817	606708.304220	40.032551
3014.318965	607691.075811	40.037568
3017.079577	608674.348795	40.042586
3020.497255	609653.224867	40.047604
3023.390447	610639.456308	40.052621
3026.209473	611605.803513	40.057639
3029.430259	612560.496250	40.062656
3031.967070	613507.867563	40.067674
3034.925590	614440.485146	40.072692
3037.689220	615390.608860	40.077709
3040.652460	616335.917611	40.082727
3043.745803	617299.073248	40.087744
3046.279199	618264.386428	40.092762
3049.074397	619232.820650	40.097780
3051.895647	620214.660672	40.102797
3054.637217	621189.327965	40.107815
3057.432701	622184.888842	40.112832
3060.410646	623185.575036	40.117850
3063.650407	624190.072610	40.122868
3066.313888	625213.257213	40.127885
3069.391553	626228.682370	40.132903
3072.543164	627262.781063	40.137920
3075.346874	628293.889843	40.142938
3078.438784	629323.952079	40.147956
3081.596127	630383.316826	40.152973
3084.408804	631435.741378	40.157991
3087.904372	632491.193470	40.163008
3090.693083	633556.091360	40.168026
3094.076274	634613.744477	40.173044
3096.846170	635699.392449	40.178061
3099.982456	636761.110760	40.183079
3103.410681	637848.371901	40.188096
3106.455216	638922.608679	40.193114
3109.699490	640005.631170	40.198132
3112.603315	641099.770167	40.203149
3116.103239	642184.665507	40.208167
3119.443541	643273.013037	40.213184
3122.745448	644366.038069	40.218202
3125.290188	645466.500057	40.223220
3128.863421	646566.922089	40.228237
3132.085843	647670.721779	40.233255
3135.317714	648766.173661	40.238272
3138.542884	649884.085883	40.243290
3141.871134	650973.996757	40.248308
3144.800981	652086.029363	40.253325
3148.390320	653199.074385	40.258343
3151.561944	654308.725083	40.263360
3154.805205	655416.894178	40.268378
3158.353930	656517.765292	40.273396
3161.504089	657627.144845	40.278413
3164.773591	658741.757101	40.283431
3168.116412	659833.823051	40.288448
3171.434739	660937.121821	40.293466
3174.542067	662041.325376	40.298484
3177.592670	663150.638543	40.303501
3181.032365	664248.561543	40.308519
3184.228879	665341.522175	40.313536
3187.032086	666457.013342	40.318554
3190.700588	667561.385420	40.323572
3194.341227	668671.056367	40.328589
3197.435078	669771.137331	40.333607
3200.606769	670860.036266	40.338624
3203.997220	671965.830783	40.343642
3207.452297	673055.125462	40.348660
3210.434480	674151.879009	40.353677
3213.493740	675240.885241	40.358695
3216.934983	676337.853208	40.363712
3219.634378	677434.814015	40.368730
3222.983744	678533.674786	40.373748
3226.229051	679641.713887	40.378765
3229.269428	680738.425234	40.383783
3232.593189	681847.179528	40.388800
3235.589133	682946.068534	40.393818
3238.599363	684033.499426	40.398836
3241.909892	685110.620594	40.403853
3244.951185	686174.947207	40.408871
3248.161099	687234.652739	40.413888
3251.297422	688313.606348	40.418906
3254.393894	689371.739262	40.423924
3257.513343	690453.714990	40.428941
3260.081630	691527.165261	40.433959
3263.134321	692600.555629	40.438976
3266.264719	693704.315140	40.443994
3269.903950	694800.660905	40.449012
3273.449391	695914.345449	40.454029
3276.023963	697027.553707	40.459047
3279.412412	698138.305406	40.464064
3282.093899	699273.178883	40.469082
3285.569335	700387.697068	40.474100
3288.746023	701532.408143	40.479117
3291.738711	702672.340400	40.484135
3295.178640	703823.793798	40.489152
3298.250001	704991.802944	40.494170
3301.509189	706150.903947	40.499188
3304.692052	707327.842512	40.504205
3307.704372	708515.048649	40.509223
3311.518273	709695.272768	40.514240
3314.254339	710894.574109	40.519258
3318.043875	712085.314735	40.524276
3321.230013	713292.718608	40.529293
3324.481533	714510.184369	40.534311
3327.915238	715701.316024	40.539328
3331.030025	716936.169435	40.544346
3334.320070	718154.536123	40.549364
3337.981673	719393.537750	40.554381
3341.041211	720627.212002	40.559399
3344.502975	721859.796178	40.564416
3347.723898	723100.097875	40.569434
3351.237527	724352.325901	40.574452
3354.531659	725600.099532	40.579469
3357.817169	726850.650076	40.584487
3361.605920	728104.336011	40.589504
3364.671619	729357.849646	40.594522
3368.292708	730613.943606	40.599540
3371.852121	731884.867323	40.604557
3375.276621	733141.293049	40.609575
3378.479741	734400.620566	40.614592
3381.740666	735669.811785	40.619610
3385.388416	736939.281164	40.624628
3388.705932	738211.860296	40.629645
3391.863309	739489.246002	40.634663
3395.415972	740762.907719	40.639680
3398.231300	742057.794762	40.644698
3401.331999	743350.449654	40.649716
3405.182316	744644.593124	40.654733
3408.643242	745934.741718	40.659751
3411.774609	747236.660743	40.664768
3414.955218	748552.646896	40.669786
3418.586241	749852.124047	40.674804
3422.208359	751168.825715	40.679821
3425.171469	752474.180298	40.684839
3428.690886	753796.016762	40.689856
3431.791536	755116.906782	40.694874
3435.312534	756431.739199	40.699892
3438.458004	757766.048106	40.704909
3441.858502	759088.219637	40.709927
3445.650710	760420.429978	40.714944
3448.714524	761756.412411	40.719962
3452.267721	763095.127323	40.724980
3455.990082	764432.346335	40.729997
3459.134952	765774.535885	40.735015
3462.422047	767080.283534	40.740020
3465.731273	768366.608607	40.745024
3469.180406	769586.710046	40.750029
3472.654471	770753.497392	40.755034
3475.732065	771855.341155	40.760039
3479.034673	772892.610884	40.765044
3481.509116	773846.301244	40.770048
3484.465421	774739.716063	40.775053
3487.457838	775571.325840	40.780058
3489.694338	776332.913054	40.785063
3492.644313	777027.506203	40.790068
3494.991728	777665.578881	40.795072
3497.081508	778232.619554	40.800077
3499.103309	778730.926543	40.805082
3501.199007	779177.074265	40.810087
3503.340138	779561.284809	40.815092
3504.830922	779917.191081	40.820096
3506.656382	780210.193200	40.825101
3508.648426	780441.556522	40.830106
3509.613438	780647.694658	40.835111
3511.382526	780785.160940	40.840116
3512.256435	780902.699365	40.845120
3513.264192	780957.880809	40.850125
3514.585955	780995.200700	40.855130
3515.617944	781012.052950	40.860135
3516.429012	780981.515447	40.865140
3517.077673	780919.764044	40.870144
3517.846427	780835.115123	40.875149
3519.030596	780722.992906	40.880154
3519.287833	780586.077288	40.885159
3520.132548	780424.560149	40.890164
3520.541217	780253.516804	40.895168
3521.053414	780059.523500	40.900173
3521.422007	779841.093753	40.905178
3522.037843	779622.026206	40.910183
3522.805068	779370.203636	40.915188
3522.974036	779120.439294	40.920192
3523.418509	778834.401049	40.925197
3523.735944	778534.100421	40.930202
3523.915601	778252.462929	40.935207
3524.419403	777935.324209	40.940212
3524.492509	777626.019410	40.945216
3524.362893	777285.823237	40.950221
3524.891373	776952.197303	40.955226
3524.594050	776615.590862	40.960231
3525.036749	776256.792222	40.965236
3525.174316	775918.408164	40.970240
3525.310165	775548.006577	40.975245
3525.304776	775183.222471	40.980250
3524.810183	774813.675346	40.985255
3525.488514	774451.253308	40.990260
3525.537236	774068.825520	40.995264
3525.316899	773686.126643	41.000269
3525.508129	773300.729791	41.005274
3525.656262	772925.761212	41.010279
3525.346348	772530.506934	41.015284
3525.191213	772139.491286	41.020288
3525.582673	771743.685157	41.025293
3525.343744	771350.621814	41.030298
3525.237201	770971.556212	41.035303
3525.444790	770563.006723	41.040308
3525.043416	770170.794168	41.045312
3524.978852	769781.363145	41.050317
3525.231207	769381.413045	41.055322
3524.879342	768986.370173	41.060327
3524.759081	768586.290752	41.065332
3524.695372	768180.217169	41.070336
3524.628089	767785.112780	41.075341
3524.243057	767386.441688	41.080346
3523.911194	767014.012699	41.085351
3524.176261	766618.643780	41.090356
3523.919793	766225.065210	41.095360
3523.783681	765832.678532	41.100365
3524.037002	765446.616280	41.105370
3523.464365	765073.538526	41.110375
3523.294275	764679.075457	41.115380
3523.335497	764300.187777	41.120384
3523.213333	763914.108391	41.125389
3523.372050	763532.253191	41.130394
3522.920143	763153.931349	41.135399
3522.670816	762773.387049	41.140404
3522.790159	762405.142455	41.145408
3522.572780	762023.223291	41.150413
3522.497760	761653.247636	41.155418
3522.193569	761289.211049	41.160423
3522.291979	760905.654084	41.165428
3521.626688	760547.906328	41.170432
3521.858495	760179.090588	41.175437
3521.884092	759808.860045	41.180442
3521.488963	759453.285599	41.185447
3521.268638	759087.599687	41.190452
3521.013002	758731.326950	41.195456
3520.730537	758382.394727	41.200461
3520.829521	758023.118839	41.205466
3520.563295	757686.489500	41.210471
3520.591627	757331.387536	41.215476
3520.118532	756985.531999	41.220480
3520.038821	756650.109411	41.225485
3520.357876	756313.372353	41.230490
3520.000979	755970.758868	41.235495
3519.682048	755629.407269	41.240500
3519.855340	755299.610105	41.245504
3519.559047	754968.049426	41.250509
3519.240991	754630.602722	41.255514
3519.254984	754311.601724	41.260519
3519.731953	753979.229017	41.265524
3519.056442	753662.487198	41.270528
3518.732402	753323.008861	41.275533
3519.240438	753004.958575	41.280538
3518.416773	752687.361489	41.285543
3518.507799	752364.316237	41.290548
3518.136441	752050.816231	41.295552
3518.299619	751736.672112	41.300557
3517.825685	751428.695462	41.305562
3517.680699	751122.628108	41.310567
3517.826198	750819.266971	41.315572
3517.367343	750524.045436	41.320576
3517.416866	750230.902481	41.325581
3517.446159	749937.060141	41.330586
3517.376668	749631.563615	41.335591
3517.151248	749337.641720	41.340596
3517.121294	749046.048058	41.345600
3516.575600	748752.107357	41.350605
3516.731692	748471.232743	41.355610
3516.450749	748191.556499	41.360615
3516.486188	747889.383686	41.365620
3515.991666	747624.052586	41.370624
3516.178713	747340.364744	41.375629
3516.008747	747062.359321	41.380634
3515.808100	746799.818127	41.385639
3515.778342	746515.444116	41.390644
3515.567732	746250.365484	41.395648
3515.496822	745984.908857	41.400653
3515.380295	745704.968100	41.405658
3515.425749	745442.489062	41.410663
3515.320926	745179.432805	41.415668
3515.011065	744919.416965	41.420672
3514.875952	744655.557181	41.425677
3515.111991	744410.957266	41.430682
3514.561718	744147.494866	41.435687
3514.545720	743893.873097	41.440692
3514.420110	743645.007623	41.445696
3514.403613	743390.183090	41.450701
3514.434278	743141.622053	41.455706
3513.866514	742893.893470	41.460711
3514.109943	742648.545292	41.465716
3513.939135	742401.873146	41.470720
3513.697019	742175.727245	41.475725
3513.619176	741926.008392	41.480730
3513.314998	741698.870005	41.485735
3513.119253	741470.718113	41.490740
3512.959578	741253.879312	41.495744
3512.939292	741015.249977	41.500749
3512.957369	740791.642892	41.505754
3512.803423	740572.657717	41.510759
3512.944366	740353.271666	41.515764
3512.391603	740133.449743	41.520768
3512.375524	739916.204416	41.525773
3512.540309	739705.106654	41.530778
3512.212325	739489.879710	41.535783
3512.434250	739271.884993	41.540788
3512.109150	739063.720118	41.545792
3511.985847	738849.579930	41.550797
3512.101616	738642.865026	41.555802
3511.732976	738451.363713	41.560807
3511.938890	738225.624981	41.565812
3511.960712	738029.002658	41.570816
3511.952484	737823.375415	41.575821
3512.038467	737615.748170	41.580826
3511.514573	737424.693083	41.585831
3511.631967	737215.516352	41.590836
3511.494883	737020.627233	41.595840
3511.175548	736822.348968	41.600845
3511.347079	736630.418031	41.605850
3510.936973	736438.726785	41.610855
3511.129315	736239.755928	41.615860
3510.818444	736060.658699	41.620864
3510.586665	735863.282530	41.625869
3510.876457	735687.443328	41.630874
3510.478354	735498.796067	41.635879
3510.664868	735314.205512	41.640884
3510.267454	735144.109907	41.645888
3510.257423	734962.117365	41.650893
3510.120532	734779.349650	41.655898
3509.752304	734607.158984	41.660903
3510.271368	734424.522610	41.665908
3509.678958	734265.132331	41.670912
3509.772536	734088.448949	41.675917
3509.742547	733928.860336	41.680922
3509.345584	733768.536972	41.685927
3509.511368	733597.721804	41.690932
3509.729154	733439.221262	41.695936
3509.635095	733257.847579	41.700941
3509.537691	733098.847708	41.705946
3509.141078	732944.201224	41.710951
3509.260825	732776.198212	41.715956
3509.212884	732634.014178	41.720960
3509.262901	732471.412922	41.725965
3508.735547	732309.794745	41.730970
3508.837174	732148.020185	41.735975
3509.163812	732003.535246	41.740980
3508.826265	731851.482347	41.745984
3508.610894	731697.178242	41.750989
3509.038259	731540.487518	41.755994
3508.282343	731404.191977	41.760999
3508.615403	731245.728452	41.766004
3508.266111	731105.597466	41.771008
3508.436819	730963.892766	41.776013
3508.339499	730818.812784	41.781018
3508.135806	730687.960583	41.786023
3508.389001	730542.421729	41.791028
3507.751830	730414.954585	41.796032
3508.140036	730272.855314	41.801037
3507.876859	730136.457264	41.806042
3507.570420	730000.955523	41.811047
3507.714879	729855.917547	41.816052
3507.849094	729737.178018	41.821056
3507.663789	729603.284108	41.826061
3507.687649	729470.195532	41.831066
3507.622475	729344.004159	41.836071
3507.787454	729202.814521	41.841076
3507.549701	729079.817480	41.846080
3507.346093	728943.290537	41.851085
3507.682823	728823.018326	41.856090
3507.465744	728702.984194	41.861095
3507.369421	728579.906768	41.866100
3507.054291	728449.086434	41.871104
3507.144425	728322.358291	41.876109
3507.444130	728199.408017	41.881114
3506.892293	728078.825408	41.886119
3507.002277	727962.838143	41.891124
3506.732213	727849.289740	41.896128
3506.974266	727737.934219	41.901133
3506.831571	727611.976515	41.906138
3506.683544	727497.362756	41.911143
3506.798566	727377.006695	41.916148
3506.925134	727267.893202	41.921152
3506.694190	727165.277817	41.926157
3506.676242	727047.861889	41.931162
3506.516041	726944.835729	41.936167
3506.406266	726833.327686	41.941172
3506.283967	726731.977149	41.946176
3506.061130	726614.142845	41.951181
3506.459488	726508.244536	41.956186
3506.473858	726403.250448	41.961191
3506.530396	726309.792915	41.966196
3506.489035	726198.463155	41.971200
3506.568810	726082.206472	41.976205
3506.461058	725966.325895	41.981210
3506.191966	725875.146847	41.986215
3506.332314	725766.704814	41.991220
3506.442134	725659.455643	41.996224
3506.350644	725555.508754	42.001229
3506.341785	725455.015703	42.006234
3506.170742	725354.052601	42.011239
3505.964978	725248.881800	42.016244
3506.063928	725147.326567	42.021248
3506.059662	725042.813708	42.026253
3506.229867	724949.867091	42.031258
3505.665615	724859.865212	42.036263
3505.966244	724749.549729	42.041268
3505.458735	724656.513231	42.046272
3505.616298	724569.660114	42.051277
3505.809874	724483.097505	42.056282
3505.518347	724375.303001	42.061287
3505.727264	724285.415246	42.066292
3505.724518	724194.272789	42.071296
3505.325421	724095.016900	42.076301
3505.758534	724013.514779	42.081306
3505.436760	723926.733866	42.086311
3505.443192	723830.827827	42.091316
3505.264896	723745.756094	42.096320
3505.045251	723651.173883	42.101325
3505.515057	723575.460457	42.106330
3505.281622	723488.709944	42.111335
3505.600399	723398.893561	42.116340
3505.386711	723321.406910	42.121344
3505.109011	723223.359695	42.126349
3504.895598	723135.660394	42.131354
3504.995159	723059.953684	42.136359
3505.018579	722969.983032	42.141364
3504.918587	722904.717216	42.146368
3504.879477	722809.897345	42.151373
3505.157516	722736.091482	42.156378
3505.138221	722658.269160	42.161383
3504.864537	722575.035198	42.166388
3504.847543	722496.665695	42.171392
3504.436636	722417.269768	42.176397
3504.979307	722342.821931	42.181402
3504.546147	722270.368412	42.186407
3504.539138	722194.175610	42.191412
3504.361882	722118.307601	42.196416
3504.403731	722049.392773	42.201421
3504.396495	721977.461402	42.206426
3504.309703	721911.788981	42.211431
3504.396519	721843.311206	42.216436
3504.488959	721769.576889	42.221440
3504.279138	721700.601476	42.226445
3504.372655	721628.501747	42.231450
3504.147213	721568.501205	42.236455
3504.464181	721496.115622	42.241460
3504.562461	721428.227463	42.246464
3504.413622	721365.138992	42.251469
3504.564113	721291.936227	42.256474
3504.127959	721226.960471	42.261479
3504.152904	721148.720049	42.266484
3504.159308	721083.224030	42.271488
3504.195494	721018.317554	42.276493
3504.564807	720953.801909	42.281498
3503.906871	720889.851671	42.286503
3504.242248	720825.489366	42.291508
3504.105122	720762.939785	42.296512
3504.372378	720695.017791	42.301517
3503.976312	720629.386180	42.306522
3503.685742	720587.090303	42.311527
3504.260093	720513.612512	42.316532
3504.129279	720450.315786	42.321536
3503.855532	720378.612809	42.326541
3504.296424	720316.658811	42.331546
3503.910145	720259.055369	42.336551
3504.161897	720192.421037	42.341556
3503.952191	720131.762911	42.346560
3503.751958	720065.896239	42.351565
3503.878833	720014.107296	42.356570
3503.822038	719951.637549	42.361575
3504.169056	719900.654604	42.366580
3503.592628	719842.187036	42.371584
3503.947322	719777.615098	42.376589
3504.118241	719719.172291	42.381594
3503.546101	719663.678053	42.386599
3503.947368	719603.312115	42.391604
3503.488846	719538.277249	42.396608
3503.420591	719488.599940	42.401613
3503.770608	719437.316131	42.406618
3503.887600	719367.523657	42.411623
3504.009669	719304.077369	42.416628
3503.854629	719254.958465	42.421632
3503.675622	719196.768018	42.426637
3503.808425	719132.078871	42.431642
3503.719868	719081.162688	42.436647
3503.908177	719022.166621	42.441652
3503.880543	718974.612028	42.446656
3503.714196	718923.360551	42.451661
3503.782764	718861.308315	42.456666
3503.931105	718796.911572	42.461671
3503.872448	718742.814403	42.466676
3503.573142	718684.045073	42.471680
3503.567676	718632.616520	42.476685
3504.088277	718571.677924	42.481690
3503.811758	718517.565597	42.486695
3503.728665	718449.881425	42.491700
3503.685475	718399.449567	42.496704
3503.807113	718339.269360	42.501709
3503.425681	718280.857899	42.506714
3503.612269	718249.283610	42.511719
3503.846043	718178.866800	42.516724
3503.738473	718127.699951	42.521728
3503.734281	718073.688671	42.526733
3503.601085	718005.513177	42.531738
3503.347330	717962.949920	42.536743
3503.685902	717908.434709	42.541748
3503.958262	717846.490161	42.546752
3503.499334	717792.849591	42.551757
3503.661613	717739.007121	42.556762
3503.486280	717679.168698	42.561767
3503.815943	717625.744323	42.566772
3503.410127	717575.218444	42.571776
3503.327364	717528.259919	42.576781
3503.552784	717479.315893	42.581786
3503.407031	717435.392917	42.586791
3503.765051	717374.918821	42.591796
3503.522261	717319.007504	42.596800
3503.744039	717272.642199	42.601805
3503.697499	717217.491513	42.606810
3503.606005	717167.109792	42.611815
3503.585615	717104.662361	42.616820
3503.612703	717051.581807	42.621824
3503.424440	716997.296292	42.626829
3503.553056	716942.214143	42.631834
3503.444539	716894.115401	42.636839
3503.318620	716844.630304	42.641844
3503.425433	716799.075010	42.646848
3503.309092	716751.075947	42.651853
3503.163250	716700.105106	42.656858
3503.286116	716651.123542	42.661863
3503.273759	716601.320660	42.666868
3503.363433	716564.100833	42.671872
3503.237341	716513.572067	42.676877
3503.445913	716457.828673	42.681882
3503.160810	716418.685651	42.686887
3503.215250	716366.935670	42.691892
3503.103609	716321.612213	42.696896
3502.886634	716281.117899	42.701901
3503.226754	716228.823911	42.706906
3503.088855	716199.775819	42.711911
3502.962490	716142.150766	42.716916
3503.002687	716097.942099	42.721920
3502.918743	716063.874071	42.726925
3503.188877	716012.483247	42.731930
3502.842558	715982.178879	42.736935
3503.246994	715930.715817	42.741940
3502.706351	715887.593962	42.746944
3502.874003	715845.198569	42.751949
3503.115987	715811.968818	42.756954
3502.736233	715780.081667	42.761959
3503.205611	715730.789589	42.766964
3503.375011	715683.134239	42.771968
3503.161152	715636.285953	42.776973
3503.212019	715583.092979	42.781978
3502.934304	715548.757115	42.786983
3503.309144	715490.548885	42.791988
3503.189873	715454.499680	42.796993
3503.164654	715398.390881	42.801997
3503.338608	715353.957813	42.807002
3503.038809	715321.410765	42.812007
3503.416162	715260.372520	42.817012
3503.356811	715222.675167	42.822017
3503.167229	715176.266854	42.827021
3503.131807	715125.169039	42.832026
3503.310621	715091.004162	42.837031
3503.384330	715027.037324	42.842036
3503.074700	714992.406752	42.847041
3502.962127	714941.965548	42.852045
3503.291440	714901.473813	42.857050
3502.804258	714861.265268	42.862055
3502.981661	714820.748559	42.867060
3502.913386	714778.287438	42.872065
3502.698583	714728.953387	42.877069
3502.876892	714695.878583	42.882074
3502.878084	714661.790853	42.887079
3502.827646	714608.955749	42.892084
3502.715187	714578.260459	42.897089
3503.187262	714540.224399	42.902093
3502.830274	714498.007914	42.907098
3502.896858	714458.549726	42.912103
3502.949254	714407.284234	42.917108
3503.004308	714372.888744	42.922113
3502.818392	714334.315117	42.927117
3503.244918	714281.052032	42.932122
3502.970409	714242.839926	42.937127
3503.026297	714196.733118	42.942132
3503.096902	714168.487217	42.947137
3502.901822	714124.207721	42.952141
3502.942410	714080.385377	42.957146
3502.710995	714040.875096	42.962151
3503.312976	713994.081743	42.967156
3502.910500	713956.137534	42.972161
3503.090670	713921.223368	42.977165
3502.969485	713875.342473	42.982170
3502.779093	713828.529894	42.987175
3503.046158	713780.152983	42.992180
3502.778513	713739.704420	42.997185
3503.118179	713706.053298	43.002189
3503.035559	713660.512249	43.007194
3502.944749	713631.298669	43.012199
3503.000641	713581.268194	43.017204
3502.780761	713538.974695	43.022209
3502.889218	713502.681126	43.027213
3502.836151	713460.359748	43.032218
3502.444403	713415.960070	43.037223
3503.048127	713375.663942	43.042228
3503.030556	713355.965466	43.047233
3502.481800	713316.652964	43.052237
3502.522983	713280.419153	43.057242
3502.623602	713238.369099	43.062247
3502.763369	713199.041856	43.067252
3502.502420	713168.365909	43.072257
3502.711851	713129.274997	43.077261
3502.623576	713091.324760	43.082266
3502.468651	713057.057772	43.087271
3502.528387	713037.445071	43.092276
3502.742229	712994.283342	43.097281
3502.473153	712946.535916	43.102285
3502.572996	712917.089944	43.107290
3502.389397	712893.943764	43.112295
3502.643216	712859.757514	43.117300
3502.395735	712823.370797	43.122305
3502.877280	712785.672703	43.127309
3502.801166	712750.845570	43.132314
3502.335919	712717.571297	43.137319
3502.289883	712681.250036	43.142324
3502.606410	712648.045196	43.147329
3502.546072	712614.455651	43.152333
3502.860977	712567.056534	43.157338
3502.326862	712552.255447	43.162343
3502.147417	712511.389434	43.167348
3502.315821	712491.360520	43.172353
3502.737816	712470.098631	43.177357
3502.452817	712427.214734	43.182362
3502.221225	712391.568012	43.187367
3502.460080	712370.584208	43.192372
3502.599140	712342.122409	43.197377
3502.320353	712304.845252	43.202381
3502.467153	712276.084165	43.207386
3502.165015	712231.415346	43.212391
3502.208174	712203.614105	43.217396
3502.449435	712172.454741	43.222401
3502.555115	712147.223915	43.227405
3502.765894	712108.376242	43.232410
3502.497797	712081.022950	43.237415
3502.697073	712034.136245	43.242420
3502.687380	712014.582254	43.247425
3502.583073	711980.352206	43.252429
3502.681490	711925.639371	43.257434
3502.486113	711899.117291	43.262439
3502.386926	711868.558886	43.267444
3502.291155	711840.332637	43.272449
3502.230318	711806.193994	43.277453
3502.519977	711773.536148	43.282458
3502.516264	711749.165960	43.287463
3502.770272	711713.386741	43.292468
3502.414016	711680.189704	43.297473
3502.272569	711657.827372	43.302477
3502.406937	711625.045637	43.307482
3502.103344	711599.235353	43.312487
3502.518916	711564.520880	43.317492
3502.432314	711534.157744	43.322497
3502.328141	711502.010476	43.327501
3502.709231	711467.301288	43.332506
3502.332074	711447.161260	43.337511
3502.591467	711400.608614	43.342516
3502.653949	711371.610175	43.347521
3502.478663	711336.197929	43.352525
3502.488084	711297.479006	43.357530
3502.623725	711283.012079	43.362535
3502.349083	711236.844358	43.367540
3502.365006	711211.129162	43.372545
3502.366726	711181.792619	43.377549
3502.564677	711147.360497	43.382554
3502.309227	711125.660851	43.387559
3502.500869	711085.769248	43.392564
3502.790077	711056.732378	43.397569
3502.415233	711024.925740	43.402573
3502.746568	710977.117941	43.407578
3502.695565	710953.547501	43.412583
3502.682637	710912.447797	43.417588
3502.517401	710883.683777	43.422593
3502.551764	710854.191806	43.427597
3502.636565	710821.415144	43.432602
3502.065241	710798.674616	43.437607
3502.198210	710758.542944	43.442612
3502.077573	710736.323682	43.447617
3502.443235	710702.457821	43.452621
3502.788672	710674.750702	43.457626
3502.192601	710644.120843	43.462631
3502.579959	710607.421458	43.467636
3502.480836	710584.602553	43.472641
3502.206479	710540.615253	43.477645
3502.485303	710514.904279	43.482650
3502.222263	710489.034298	43.487655
3502.287633	710445.536598	43.492660
3502.480612	710421.576986	43.497665
3502.141803	710386.435945	43.502669
3502.482356	710366.125452	43.507674
3502.373109	710335.463910	43.512679
3502.256911	710308.477030	43.517684
3502.543475	710265.488046	43.522689
3502.526801	710241.165320	43.527693
3501.986205	710219.212481	43.532698
3502.018682	710183.761207	43.537703
3502.168714	710156.630691	43.542708
3502.094903	710129.090169	43.547713
3501.883527	710110.160769	43.552717
3502.353489	710081.190087	43.557722
3502.564782	710056.581049	43.562727
3502.419436	710024.782503	43.567732
3502.752259	710003.777389	43.572737
3502.417392	709978.662373	43.577741
3502.313335	709935.239634	43.582746
3502.071508	709912.492088	43.587751
3502.415777	709881.654898	43.592756
3501.991384	709843.298723	43.597761
3502.042743	709816.133738	43.602765
3502.230776	709787.258161	43.607770
3501.884051	709767.704895	43.612775
3502.089270	709740.216436	43.617780
3502.368449	709721.801108	43.622785
3502.052516	709694.448019	43.627789
3502.505220	709658.974972	43.632794
3502.388554	709639.879980	43.637799
3502.302501	709609.013416	43.642804
3502.211323	709590.807772	43.647809
3502.318639	709557.873604	43.652813
3502.471723	709522.201119	43.657818
3501.880081	709499.559759	43.662823
3502.266417	709467.671531	43.667828
3502.277127	709429.936884	43.672833
3502.232815	709420.064130	43.677837
3502.223704	709385.261828	43.682842
3502.197484	709361.037466	43.687847
3502.564150	709334.464434	43.692852
3502.182005	709294.460405	43.697857
3502.284192	709282.031229	43.702861
3502.483670	709238.753534	43.707866
3502.084946	709219.952326	43.712871
3502.529226	709192.670968	43.717876
3502.363024	709171.249536	43.722881
3502.273850	709137.601372	43.727885
3502.687838	709103.324013	43.732890
3502.172211	709087.620111	43.737895
3502.342576	709044.048324	43.742900
3502.392172	709020.207712	43.747905
3502.422618	708994.036581	43.752909
3502.538957	708946.451450	43.757914
3502.548975	708936.867095	43.762919
3502.559912	708889.646575	43.767924
3502.418492	708869.858815	43.772929
3502.468700	708833.008761	43.777933
3502.818031	708791.888811	43.782938
3502.687022	708765.793238	43.787943
3502.265727	708728.623204	43.792948
3502.514542	708698.095397	43.797953
3502.466969	708665.084008	43.802957
3502.578346	708623.059046	43.807962
3502.255576	708598.881388	43.812967
3502.638230	708564.408424	43.817972
3502.701639	708530.087231	43.822977
3502.556571	708503.744906	43.827981
3502.451021	708461.605932	43.832986
3502.197245	708436.721288	43.837991
3502.595003	708411.034053	43.842996
3502.531256	708374.449076	43.848001
3502.078227	708351.732171	43.853005
3502.615168	708318.573482	43.858010
3502.498663	708283.238187	43.863015
3502.481097	708256.675472	43.868020
3502.341371	708228.444510	43.873025
3502.711770	708195.561065	43.878029
3502.657521	708160.910190	43.883034
3502.484767	708125.583514	43.888039
3502.555440	708095.927073	43.893044
3502.786140	708068.031799	43.898049
3502.343385	708029.422222	43.903053
3502.570960	707991.893789	43.908058
3502.652061	707968.640944	43.913063
3502.936625	707925.739857	43.918068
3502.792797	707890.010184	43.923073
3502.521851	707839.552920	43.928077
3502.952697	707813.361868	43.933082
3502.477393	707782.602511	43.938087
3502.810078	707738.947688	43.943092
3502.466742	707713.281162	43.948097
3502.557634	707673.886832	43.953101
3502.705629	707635.476094	43.958106
3502.600682	707609.074748	43.963111
3502.594350	707572.675528	43.968116
3502.922699	707547.344766	43.973121
3502.549034	707514.084717	43.978125
3502.733686	707462.904592	43.983130
3502.478691	707427.787231	43.988135
3502.790656	707401.813157	43.993140
3502.636634	707361.613522	43.998145
3502.387375	707330.864958	44.003149
3502.345119	707283.594698	44.008154
3502.460212	707263.363671	44.013159
3502.327209	707227.232165	44.018164
3502.572205	707202.162428	44.023169
3502.145950	707176.756265	44.028173
3502.623475	707143.503514	44.033178
3502.130883	707114.780747	44.038183
3502.315073	707083.562581	44.043188
3502.351049	707049.339313	44.048193
3502.404797	707017.248474	44.053197
3502.387351	706988.546320	44.058202
3502.211733	706968.660479	44.063207
3502.306283	706934.824407	44.068212
3502.600301	706914.165773	44.073217
3502.122207	706877.841341	44.078221
3502.141751	706851.864126	44.083226
3502.280741	706823.830937	44.088231
3502.357809	706799.830638	44.093236
3502.203137	706774.328870	44.098241
3502.049853	706750.316724	44.103245
3502.113687	706712.412373	44.108250
3502.191885	706693.229038	44.113255
3502.107480	706662.152930	44.118260
3502.215810	706648.576642	44.123265
3502.388423	706612.044540	44.128269
3502.331043	706588.016138	44.133274
3501.903535	706563.204346	44.138279
3502.407476	706533.024135	44.143284
3502.402976	706503.970573	44.148289
3502.201543	706479.121288	44.153293
3502.325988	706441.454085	44.158298
3502.297986	706424.174958	44.163303
3502.160794	706392.758912	44.168308
3502.531120	706360.961128	44.173313
3502.341143	706338.344538	44.178317
3502.282644	706295.442182	44.183322
3502.160690	706273.261214	44.188327
3502.222408	706238.235808	44.193332
3502.217437	706214.793735	44.198337
3502.216068	706189.811315	44.203341
3502.347704	706164.757239	44.208346
3502.325502	706144.893881	44.213351
3502.228806	706101.748515	44.218356
3502.436440	706079.413406	44.223361
3502.414780	706054.483605	44.228365
3502.326112	706020.723799	44.233370
3502.368417	705994.541574	44.238375
3502.465920	705956.231000	44.243380
3502.149397	705943.816319	44.248385
3502.284406	705910.714591	44.253389
3502.749679	705868.270166	44.258394
3502.099871	705849.204907	44.263399
3502.233589	705829.811826	44.268404
3502.502033	705794.353198	44.273409
3502.150355	705765.006661	44.278413
3501.965971	705729.672049	44.283418
3502.151234	705708.581419	44.288423
3502.009368	705677.064192	44.293428
3502.242173	705664.260572	44.298433
3501.838430	705633.481721	44.303437
3502.126920	705611.728128	44.308442
3502.181453	705582.363707	44.313447
3502.295452	705561.830842	44.318452
3502.366299	705530.278030	44.323457
3501.964376	705510.128077	44.328461
3502.003822	705467.056445	44.333466
3502.014868	705459.504578	44.338471
3501.922790	705419.484351	44.343476
3502.152565	705413.883279	44.348481
3501.885974	705383.279623	44.353485
3501.870012	705357.552115	44.358490
3501.553261	705338.629532	44.363495
3501.803805	705314.944223	44.368500
3502.072520	705295.726389	44.373505
3502.154599	705269.684430	44.378509
3502.306843	705253.565402	44.383514
3501.950703	705232.612491	44.388519
3501.964702	705202.955421	44.393524
3502.174023	705175.451692	44.398529
3501.295725	705163.029100	44.403533
3502.001049	705134.301026	44.408538
3501.960290	705108.924577	44.413543
3501.877161	705099.748682	44.418548
3501.653343	705080.412830	44.423553
3501.971563	705050.506415	44.428557
3502.310213	705034.703984	44.433562
3502.077569	705018.945983	44.438567
3501.920325	704992.445879	44.443572
3502.074254	704968.874891	44.448577
3501.837129	704936.724887	44.453581
3501.945726	704911.969021	44.458586
3501.826452	704899.768706	44.463591
3502.207164	704879.985072	44.468596
3501.948188	704852.209751	44.473601
3502.082627	704818.011077	44.478605
3502.133396	704790.432897	44.483610
3501.990270	704776.497696	44.488615
3501.953165	704740.687687	44.493620
3501.956578	704716.296323	44.498625
3501.865719	704704.140726	44.503629
3501.946168	704677.302435	44.508634
3502.226213	704670.301669	44.513639
3501.863838	704642.145300	44.518644
3501.777204	704618.364613	44.523649
3501.992645	704593.341848	44.528653
3502.148299	704567.484358	44.533658
3502.035935	704548.079272	44.538663
3502.068645	704528.600562	44.543668
3502.134748	704500.969256	44.548673
3502.013491	704471.530672	44.553677
3501.919314	704445.465595	44.558682
3502.071165	704425.370892	44.563687
3502.174956	704400.713711	44.568692
3502.257023	704379.587168	44.573697
3502.179844	704356.499693	44.578701
3502.380488	704318.959713	44.583706
3502.002197	704312.961342	44.588711
3502.114678	704277.422838	44.593716
3501.871934	704263.254830	44.598721
3501.948228	704228.020157	44.603725
3502.175064	704217.401247	44.608730
3502.006362	704190.304427	44.613735
3501.945637	704156.979841	44.618740
3501.977288	704135.513255	44.623745
3501.835137	704121.080043	44.628749
3502.237705	704102.135584	44.633754
3502.006960	704085.133578	44.638759
3501.704346	704067.646584	44.643764
3501.851473	704024.997144	44.648769
3502.128299	704006.222234	44.653773
3502.171541	703982.865521	44.658778
3502.012618	703964.460400	44.663783
3502.322294	703928.887975	44.668788
3502.182556	703911.125425	44.673793
3501.985351	703880.852777	44.678797
3502.165589	703845.500060	44.683802
3502.221528	703830.984044	44.688807
3501.905730	703803.761207	44.693812
3502.217796	703773.056501	44.698817
3501.862673	703763.625916	44.703821
3502.072095	703738.253907	44.708826
3502.026644	703712.476683	44.713831
3501.996486	703687.690500	44.718836
3502.063228	703661.050047	44.723841
3501.841864	703641.263431	44.728845
3502.126180	703606.240366	44.733850
3501.939635	703596.384362	44.738855
3501.963332	703568.359611	44.743860
3501.873744	703543.831221	44.748865
3501.994852	703524.931881	44.753869
3502.220104	703499.407517	44.758874
3501.847226	703487.495410	44.763879
3501.847895	703457.138994	44.768884
3502.201068	703439.244576	44.773889
3502.069624	703417.405620	44.778893
3501.821124	703395.635579	44.783898
3501.959099	703375.341997	44.788903
3501.673494	703336.983582	44.793908
3501.736962	703336.526010	44.798913
3501.955581	703306.033786	44.803917
3502.290614	703285.260367	44.808922
3501.839856	703266.951534	44.813927
3501.829164	703226.709016	44.818932
3501.846794	703214.732189	44.823937
3501.413227	703203.028427	44.828941
3501.919896	703180.785625	44.833946
3501.938580	703163.293546	44.838951
3501.979575	703124.731324	44.843956
3502.088718	703117.757472	44.848961
3501.974754	703094.573325	44.853965
3501.969840	703066.800095	44.858970
3501.968913	703047.025486	44.863975
3502.074042	703016.749689	44.868980
3502.166628	702998.946989	44.873985
3501.892404	702977.627309	44.878989
3502.293960	702958.581156	44.883994
3502.109393	702931.035837	44.888999
3501.952951	702902.343011	44.894004
3502.034968	702871.822086	44.899009
3501.887577	702859.126661	44.904013
3502.329345	702836.943363	44.909018
3501.855224	702817.792754	44.914023
3501.754750	702780.047300	44.919028
3501.729817	702762.362853	44.924033
3501.568161	702746.141828	44.929037
3501.647246	702708.962725	44.934042
3501.853866	702701.873104	44.939047
3501.758489	702692.646986	44.944052
3501.719642	702662.741492	44.949057
3501.737558	702651.310405	44.954061
3502.065572	702643.455418	44.959066
3502.176609	702623.164518	44.964071
3502.134950	702610.252556	44.969076
3502.290187	702571.967185	44.974081
3502.121596	702557.436348	44.979085
3501.886611	702517.475944	44.984090
3502.110177	702510.830572	44.989095
3501.911932	702469.075103	44.994100
3502.210080	702457.498210	44.999105
3501.830219	702424.169864	45.004109
3501.956103	702407.503315	45.009114
3501.940924	702392.996614	45.014119
3502.156813	702360.762403	45.019124
3502.235936	702340.177966	45.024129
3501.955126	702306.634090	45.029133
3502.114700	702288.222621	45.034138
3501.931357	702273.842810	45.039143
3501.560722	702248.412960	45.044148
3502.066628	702221.447282	45.049153
3501.846836	702207.769030	45.054157
3501.934701	702181.120559	45.059162
3501.707694	702164.660763	45.064167
3501.965781	702140.319574	45.069172
3502.203573	702108.528038	45.074177
3501.999981	702100.014793	45.079181
3502.429419	702071.371761	45.084186
3501.679426	702058.824148	45.089191
3501.985984	702027.319131	45.094196
3502.212850	702006.858636	45.099201
3501.708046	701973.797606	45.104205
3502.026331	701945.420932	45.109210
3502.001764	701936.977413	45.114215
3501.940824	701907.569882	45.119220
3501.839737	701892.629274	45.124225
3502.046752	701871.227582	45.129229
3502.031745	701843.402416	45.134234
3501.888393	701834.382061	45.139239
3502.223980	701807.542554	45.144244
3502.205177	701789.060037	45.149249
3501.660692	701754.414544	45.154253
3502.102854	701729.346179	45.159258
3501.923471	701709.945786	45.164263
3501.787174	701678.810639	45.169268
3502.255021	701677.839112	45.174273
3502.186970	701646.145977	45.179277
3501.735506	701623.361371	45.184282
3501.888156	701598.787576	45.189287
3502.109161	701574.798777	45.194292
3502.090440	701542.152951	45.199297
3502.459434	701534.240524	45.204301
3502.572803	701496.702738	45.209306
3502.461865	701471.873852	45.214311
3502.207928	701433.203647	45.219316
3502.399900	701408.473753	45.224321
3502.376784	701382.487161	45.229325
3502.316663	701337.473329	45.234330
3502.169667	701331.037205	45.239335
3502.309248	701296.227478	45.244340
3502.112578	701279.512530	45.249345
3502.109389	701239.657151	45.254349
3502.309524	701211.049080	45.259354
3501.974728	701184.864775	45.264359
3502.179162	701164.107825	45.269364
3502.251073	701131.594617	45.274369
3501.946367	701112.710507	45.279373
3502.404043	701080.133546	45.284378
3502.029249	701063.944501	45.289383
3502.054876	701036.259154	45.294388
3502.079244	701006.238162	45.299393
3502.210858	700991.009179	45.304397
3502.428220	700965.031417	45.309402
3502.048756	700944.817432	45.314407
3502.023710	700917.835823	45.319412
3502.350406	700892.386504	45.324417
3501.970715	700861.089749	45.329421
3502.490186	700829.893217	45.334426
3502.076905	700812.268799	45.339431
3501.976366	700780.826363	45.344436
3502.199969	700753.554785	45.349441
3502.086699	700731.606692	45.354445
3502.308884	700696.035482	45.359450
3501.755901	700678.185317	45.364455
3502.058083	700662.778561	45.369460
3501.895651	700632.389470	45.374465
3501.763903	700613.624877	45.379469
3502.076328	700590.860798	45.384474
3502.126325	700574.899047	45.389479
3502.095620	700549.308821	45.394484
3502.203472	700514.252707	45.399489
3502.054477	700501.703205	45.404493
3502.135109	700466.750787	45.409498
3501.897677	700450.090664	45.414503
3501.973285	700424.383155	45.419508
3501.946979	700399.636673	45.424513
3501.736238	700380.735493	45.429517
3502.205435	700348.004808	45.434522
3502.120374	700329.679220	45.439527
3501.902729	700302.628044	45.444532
3502.019909	700285.760075	45.449537
3501.430407	700260.559284	45.454541
3502.083164	700238.980748	45.459546
3501.929815	700215.397812	45.464551
3502.005689	700194.510640	45.469556
3502.201080	700184.190217	45.474561
3502.021397	700159.368924	45.479565
3502.028354	700142.667946	45.484570
3501.562381	700116.402642	45.489575
3501.653663	700101.228459	45.494580
3502.164939	700092.893673	45.499585
3501.952941	700062.510766	45.504589
3502.263731	700040.590470	45.509594
3501.896342	700006.654383	45.514599
3501.860154	699993.290318	45.519604
3502.101556	699962.882061	45.524609
3502.289857	699941.429027	45.529613
3502.409724	699900.901125	45.534618
3502.002948	699888.442919	45.539623
3502.166688	699853.921690	45.544628
3502.224054	699827.121951	45.549633
3501.577407	699811.124482	45.554637
3501.969958	699777.310809	45.559642
3501.799075	699770.827763	45.564647
3501.958095	699746.396826	45.569652
3501.914918	699729.255982	45.574657
3501.919112	699694.213664	45.579661
3502.035692	699681.519815	45.584666
3501.990063	699657.321169	45.589671
3502.242408	699634.166867	45.594676
3501.973587	699604.338486	45.599681
3501.534523	699592.481639	45.604685
3501.745151	699573.111641	45.609690
3501.790251	699551.184195	45.614695
3501.806833	699528.714632	45.619700
3502.123069	699515.192356	45.624705
3501.469765	699488.061327	45.629709
3501.831620	699469.411769	45.634714
3501.674075	699447.616865	45.639719
3501.535021	699429.149169	45.644724
3502.125783	699403.552605	45.649729
3501.896316	699390.169759	45.654733
3502.057628	699366.184743	45.659738
3502.041624	699349.336916	45.664743
3501.998941	699329.163107	45.669748
3501.955033	699316.395761	45.674753
3501.883825	699287.527873	45.679757
3501.994140	699267.676662	45.684762
3502.014091	699243.366653	45.689767
3502.027240	699220.548915	45.694772
3502.095270	699191.956015	45.699777
3501.581449	699178.768821	45.704781
3502.243045	699148.039967	45.709786
3501.742906	699126.201297	45.714791
3501.694390	699106.375891	45.719796
3501.928389	699083.919072	45.724801
3501.632492	699065.078787	45.729805
3502.011324	699051.396361	45.734810
3501.682226	699030.622851	45.739815
3501.730079	699013.664441	45.744820
3502.072719	698975.481559	45.749825
3501.513739	698892.609546	45.754829
3501.526440	698756.850791	45.759834
3501.290537	698590.956469	45.764839
3501.441935	698342.672096	45.769844
3501.516236	698038.813374	45.774849
3500.953803	697703.578986	45.779853
3500.727252	697277.342237	45.784858
3500.627316	696808.801333	45.789863
3500.234167	696289.565692	45.794868
3499.998562	695688.671584	45.799873
3499.441621	695067.947081	45.804877
3499.067036	694357.030244	45.809882
3498.543201	693613.352958	45.814887
3498.271479	692804.706823	45.819892
3498.022089	691938.723647	45.824897
3496.853525	691017.830717	45.829901
3496.646815	690029.410900	45.834906
3496.007994	688989.546796	45.839911
3494.768327	687891.430092	45.844916
3494.291885	686739.095913	45.849921
3493.404343	685539.089821	45.854925
3492.382819	684261.025318	45.859930
3491.696628	682935.866649	45.864935
3490.886375	681545.042534	45.869940
3489.959054	680111.586192	45.874945
3488.646173	678616.291830	45.879949
3488.069638	677066.968039	45.884954
3486.842037	675459.830439	45.889959
3485.672441	673805.649887	45.894964
3484.470135	672076.697725	45.899969
3483.304844	670301.495639	45.904973
3482.094611	668484.421671	45.909978
3480.881875	666616.018261	45.914983
3479.615398	664685.787623	45.919988
3477.938263	662694.950987	45.924993
3476.311088	660664.062223	45.929997
3475.012313	658591.654734	45.935002
3473.768641	656474.653546	45.940007
3471.538798	654292.375672	45.945012
3470.158523	652063.262879	45.950017
3468.405398	649813.922828	45.955021
3466.964533	647484.503447	45.960026
3465.314968	645131.931786	45.965031
3463.510974	642719.032149	45.970036
3461.582618	640266.518054	45.975041
3459.704779	637781.290573	45.980045
3458.018352	635241.438819	45.985050
3455.800201	632659.460080	45.990055
3453.858668	630049.764264	45.995060
3452.129760	627374.836904	46.000065
3449.879875	624681.040270	46.005069
3448.073484	621931.830547	46.010074
3445.517645	619159.493353	46.015079
3443.706952	616338.053664	46.020084
3441.434959	613480.816414	46.025089
3439.392734	610593.063368	46.030093
3436.866513	607650.763669	46.035098
3434.298630	604685.273306	46.040103
3431.901363	601691.125253	46.045108
3429.955034	598653.045033	46.050113
3427.049557	595583.191151	46.055117
3424.484139	592483.743644	46.060122
3422.203013	589353.038448	46.065127
3419.609497	586187.187074	46.070132
3417.128212	582977.704571	46.075137
3414.405062	579766.212252	46.080141
3412.060261	576499.346281	46.085146
3409.146948	573231.518069	46.090151
3406.245817	569908.890763	46.095156
3403.944406	566565.364912	46.100161
3400.709859	563204.208268	46.105165
3398.222540	559795.323231	46.110170
3395.429971	556369.639035	46.115175
3392.438445	552928.244628	46.120180
3389.359891	549444.103087	46.125185
3386.376155	545965.564659	46.130189
3383.445860	542436.269915	46.135194
3380.807466	538904.528369	46.140199
3377.612601	535330.377206	46.145204
3374.899178	531740.525561	46.150209
3371.393895	528127.460427	46.155213
3368.587639	524495.425329	46.160218
3365.501699	520850.085595	46.165223
3362.064620	517177.462845	46.170228
3358.907374	513478.255032	46.175233
3355.787046	509778.778069	46.180237
3352.443142	506042.032763	46.185242
3349.261899	502293.832173	46.190247
3346.038251	498530.574532	46.195252
3342.826896	494739.810024	46.200257
3339.539519	490960.155485	46.205261
3335.938756	487135.292519	46.210266
3332.658973	483323.466677	46.215271
3328.944922	479484.674798	46.220276
3326.115735	475624.014217	46.225281
3322.287395	471764.995323	46.230285
3318.984446	467889.904005	46.235290
3315.111016	464004.297397	46.240295
3311.751969	460098.071602	46.245300
3308.220589	456193.140620	46.250305
3304.393161	452275.242869	46.255309
3301.097684	448348.813812	46.260314
3297.731719	444406.101761	46.265319
3293.857499	440462.556602	46.270324
3290.277963	436502.332092	46.275329
3286.504594	432550.635642	46.280333
3282.725497	428592.940072	46.285338
3278.818210	424616.688687	46.290343
3275.487822	420639.719962	46.295348
3271.541696	416658.589853	46.300353
3267.755005	412671.940130	46.305357
3264.029115	408671.673121	46.310362
3260.057365	404689.779087	46.315367
3256.432345	400697.425524	46.320372
3252.814841	396696.102734	46.325377
3248.804657	392693.436368	46.330381
3245.149837	388693.080018	46.335386
3241.426720	384681.851910	46.340391
3237.269418	380671.162381	46.345396
3233.874685	376673.085056	46.350401
3229.692230	372662.417451	46.355405
3225.771829	368646.856143	46.360410
3221.701602	364644.668159	46.365415
3217.760735	360649.061704	46.370420
3213.872672	356640.378031	46.375425
3209.949940	352642.379723	46.380429
3206.160799	348642.565376	46.385434
3202.106676	344655.112599	46.390439
3197.840818	340657.994157	46.395444
3194.355309	336669.612292	46.400449
3189.947897	332674.562032	46.405453
3186.348750	328676.492035	46.410458
3181.910238	324702.747285	46.415463
3177.931376	320724.266543	46.420468
3174.084065	316752.218042	46.425473
3170.447213	312793.173729	46.430477
3166.457122	308830.083623	46.435482
3161.903553	304879.470652	46.440487
3157.952070	300929.217512	46.445492
3154.194352	296998.020612	46.450497
3150.069420	293065.159568	46.455501
3146.116981	289130.203588	46.460506
3142.262952	285204.970383	46.465511
3138.209178	281283.616457	46.470516
3133.872749	277364.871683	46.475521
3129.641360	273471.047537	46.480525
3125.903150	269569.191154	46.485530
3121.916773	265687.173779	46.490535
3117.692432	261808.759813	46.495540
3113.734005	257937.293238	46.500545
3109.325478	254085.997000	46.505549
3105.486398	250220.971614	46.510554
3101.204207	246390.125117	46.515559
3097.126807	242555.977160	46.520564
3092.904943	238728.938876	46.525569
3088.806697	234921.203365	46.530573
3084.625386	231112.469740	46.535578
3080.694525	227326.022784	46.540583
3076.384216	223548.990946	46.545588
3072.298879	219785.182826	46.550593
3068.608831	216033.461688	46.555597
3064.054160	212274.161320	46.560602
3060.239232	208447.377104	46.565607
3055.729692	204732.792713	46.570612
3051.789720	201021.325070	46.575617
3047.668879	197324.705498	46.580621
3044.086548	193626.292208	46.585626
3039.504623	189945.390926	46.590631
3035.194886	186287.871368	46.595636
3031.644049	182625.907199	46.600641
3027.328472	178991.878810	46.605645
3023.154170	175346.874620	46.610650
3018.966509	171727.485999	46.615655
3014.867518	168122.990564	46.620660
3010.651634	164511.271306	46.625665
3006.385711	160950.025528	46.630669
3002.636386	157378.148823	46.635674
2998.096279	153827.460104	46.640679
2993.660919	150281.451687	46.645684
2989.994424	146761.193782	46.650689
2985.737488	143253.984405	46.655693
2981.603337	139754.793204	46.660698
2977.339791	136271.754115	46.665703
2973.383058	132805.359929	46.670708
2968.950922	129350.432714	46.675713
2964.709517	125921.456562	46.680717
2960.504627	122488.994647	46.685722
2956.649840	119094.116275	46.690727
2952.049371	115695.093756	46.695732
2948.116109	112325.337266	46.700737
2943.586862	108970.030881	46.705741
2939.516668	105619.100542	46.710746
2935.542481	102297.491980	46.715751
2930.599995	98977.838092	46.720756
2926.615478	95695.103054	46.725761
2922.273135	92431.933731	46.730765
2917.893232	89178.247286	46.735770
2913.867106	85953.795942	46.740775
2909.449152	82743.958086	46.745780
2905.377917	79543.800573	46.750785
2900.736383	76384.278167	46.755789
2896.395386	73223.677315	46.760794
2892.284363	70094.488482	46.765799
2887.677107	66993.504274	46.770804
2883.068702	63904.515627	46.775809
2878.664463	60850.625815	46.780813
2873.908749	57817.776972	46.785818
2869.248735	54812.728211	46.790823
2864.162879	51838.840861	46.795828
2859.377281	48896.519759	46.800833
2853.985397	46008.786706	46.805837
2848.616949	43151.715230	46.810842
2841.986041	40373.072628	46.815847
2833.250504	37705.961523	46.820852
2823.443647	35142.760918	46.825857
2813.668021	32679.528948	46.830861
2804.522994	30313.769711	46.835866
2795.403044	28068.996555	46.840871
2786.766901	25951.383597	46.845876
2779.114835	23948.488138	46.850881
2771.154172	22062.480561	46.855885
2763.867831	20278.480382	46.860890
2756.629761	18610.939797	46.865895
2749.815627	17035.484046	46.870900
2743.752907	15553.130754	46.875905
2737.317011	14162.846807	46.880909
2731.538034	12837.046028	46.885914
2726.224511	11614.908046	46.890919
2720.164222	10437.148366	46.895924
2714.856931	9341.000607	46.900929
2709.723324	8309.327121	46.905933
2704.842381	7329.329828	46.910938
2699.710301	6399.676996	46.915943
2695.017686	5530.430746	46.920948
2689.760951	4715.298349	46.925953
2683.322077	3971.626889	46.930957
2677.711061	3296.440113	46.935962
2671.480364	2669.373946	46.940967
2665.410121	2118.699095	46.945972
2659.829699	1614.733593	46.950977
2654.146132	1167.111617	46.955981
2648.783359	778.406002	46.960986
2643.469134	447.575431	46.965991
2637.067282	210.243290	46.970996
2622.769393	221.779315	46.976001
2614.059993	228.810426	46.981005
2610.311231	223.147743	46.986010
2608.619360	217.228509	46.991015
2607.886370	228.191809	46.996020
2607.777737	221.145764	47.001025
2606.594481	232.618903	47.006029
2604.569477	221.552542	47.011034
2602.079518	224.378545	47.016039
2599.388726	223.285351	47.021044
2596.244242	206.909191	47.026049
2592.600245	217.310328	47.031053
2589.203664	216.629232	47.036058
2586.320626	207.205266	47.041063
2582.956660	217.335228	47.046068
2580.684689	213.125199	47.051073
2577.149781	218.842621	47.056077
2573.888619	207.586398	47.061082
2570.517081	212.909215	47.066087
2567.014369	222.161227	47.071092
2563.869950	209.905553	47.076097
2560.432073	213.898790	47.081101
2557.447483	207.948222	47.086106
2554.602275	209.442018	47.091111
2550.899612	210.023528	47.096116
2547.885971	207.311974	47.101121
2543.763205	206.473099	47.106125
2540.780113	209.507996	47.111130
2537.810394	208.963694	47.116135
2534.151420	211.182247	47.121140
2531.412137	200.104171	47.126145
2527.253106	210.839587	47.131149
2524.015361	205.757284	47.136154
2520.670203	204.132947	47.141159
2516.919864	202.686588	47.146164
2514.276495	198.738587	47.151169
2510.545444	203.826342	47.156173
2507.089685	206.404082	47.161178
2503.736472	198.479813	47.166183
2499.949143	207.570440	47.171188
2497.102822	208.657931	47.176193
2493.765163	213.161372	47.181197
2490.471524	203.552252	47.186202
2486.271583	201.242756	47.191207
2482.235588	198.714982	47.196212
2480.270711	199.825330	47.201217
2476.523356	208.436549	47.206221
2472.568370	189.435463	47.211226
2469.148044	193.404940	47.216231
2465.874602	201.311584	47.221236
2462.790664	197.005734	47.226241
2459.303369	198.711335	47.231245
2455.693100	195.203973	47.236250
2451.558350	196.533751	47.241255
2448.482819	192.398408	47.246260
2445.559854	193.674407	47.251265
2442.213941	196.512110	47.256269
2438.216145	186.128277	47.261274
2435.043892	185.362703	47.266279
2431.401730	187.148943	47.271284
2427.861153	189.156409	47.276289
2424.765360	190.393062	47.281293
2421.394283	187.378670	47.286298
2417.891650	185.383154	47.291303
2413.831149	193.777910	47.296308
2410.338210	186.620952	47.301313
2407.096543	187.120159	47.306317
2403.666238	182.419421	47.311322
2400.199453	180.211584	47.316327
2396.520392	195.282744	47.321332
2393.514880	180.748699	47.326337
2389.442753	179.621571	47.331341
2386.255303	177.621415	47.336346
2382.889865	188.564953	47.341351
2379.447811	190.513367	47.346356
2376.434401	184.474541	47.351361
2372.328324	185.718939	47.356365
2369.063589	185.567797	47.361370
2365.400719	186.336861	47.366375
2361.965083	192.081243	47.371380
2358.470874	187.416542	47.376385
2355.139842	188.185696	47.381389
2351.491533	190.616927	47.386394
2348.216514	192.996408	47.391399
2345.226840	191.095451	47.396404
2341.422588	187.904173	47.401409
2337.646740	190.764961	47.406413
2333.947572	199.701425	47.411418
2330.589096	189.450734	47.416423
2326.767861	199.167506	47.421428
2323.871774	190.665883	47.426433
2320.582202	189.115985	47.431437
2316.960100	187.012389	47.436442
2313.342960	189.556116	47.441447
2309.834593	186.269051	47.446452
2306.144161	184.417893	47.451457
2302.362848	195.339359	47.456461
2299.161405	185.785825	47.461466
2295.816020	178.495078	47.466471
2292.493357	186.557550	47.471476
2289.211228	184.598347	47.476481
2285.603232	191.740179	47.481485
2281.917775	180.566288	47.486490
2278.488686	184.285923	47.491495
2274.362232	186.958951	47.496500
2271.355862	184.788865	47.501505
2267.635519	186.601745	47.506509
2264.331510	190.378888	47.511514
2261.082091	184.270764	47.516519
2257.662708	188.264890	47.521524
2253.988365	182.204625	47.526529
2250.189832	186.503881	47.531533
2247.393674	181.346116	47.536538
2243.816741	183.538305	47.541543
2240.024321	179.697883	47.546548
2236.593196	171.971405	47.551553
2232.682266	181.462482	47.556557
2229.006738	181.866092	47.561562
2225.786680	175.564099	47.566567
2222.157742	185.707605	47.571572
2219.177581	169.245064	47.576577
2215.757393	179.138609	47.581581
2212.214189	172.721057	47.586586
2208.558625	177.458314	47.591591
2204.669662	182.583005	47.596596
2202.053193	176.927119	47.601601
2198.543843	180.639337	47.606605
2194.963837	188.783629	47.611610
2191.019739	182.716251	47.616615
2187.347246	187.891453	47.621620
2184.255085	184.865123	47.626625
2180.663306	180.690087	47.631629
2176.939654	184.347717	47.636634
2173.359105	179.222420	47.641639
2170.212222	180.770581	47.646644
2166.792141	177.465299	47.651649
2162.902019	179.072837	47.656653
2159.536644	176.699244	47.661658
2156.521805	170.874725	47.666663
2152.737004	172.048692	47.671668
2149.627716	163.012096	47.676673
2145.621148	171.019045	47.681677
2142.273656	182.291677	47.686682
2138.765018	169.566843	47.691687
2134.887414	177.593555	47.696692
2131.648812	179.254765	47.701697
2128.365928	174.518843	47.706701
2124.522235	179.763007	47.711706
2121.230147	176.468001	47.716711
2117.442731	173.515276	47.721716
2114.086157	167.339119	47.726721
2110.756739	181.876718	47.731725
2107.392818	171.737627	47.736730
2103.870237	177.863776	47.741735
2099.991432	176.805810	47.746740
2096.902298	174.303174	47.751745
2092.874870	174.446094	47.756749
2089.339642	163.654491	47.761754
2086.212338	168.770912	47.766759
2082.341510	167.786042	47.771764
2079.669171	161.728009	47.776769
2076.252978	164.632806	47.781773
2072.065974	168.020693	47.786778
2068.947366	167.192826	47.791783
2064.989716	170.191978	47.796788
2061.671322	170.932798	47.801793
2058.744744	160.884141	47.806797
2054.609222	171.448454	47.811802
2051.283826	162.914324	47.816807
2047.607588	168.605292	47.821812
2044.435527	166.834897	47.826817
2040.340565	169.805041	47.831821
2036.985015	167.184031	47.836826
2034.073507	164.430493	47.841831
2030.340999	167.850910	47.846836
2027.045441	160.064130	47.851841
2023.386011	164.390305	47.856845
2019.562565	171.177153	47.861850
2016.108802	161.615790	47.866855
2012.782319	161.374246	47.871860
2009.202679	155.649028	47.876865
2005.688848	171.742952	47.881869
2002.158437	162.761804	47.886874
1998.734966	167.747215	47.891879
1994.888111	161.872349	47.896884
1992.176823	165.254187	47.901889
1988.285392	160.610584	47.906893
1984.818685	162.802117	47.911898
1981.262124	158.154920	47.916903
1977.532697	164.581716	47.921908
1974.421827	163.225541	47.926913
1971.270832	167.347014	47.931917
1967.806418	164.427897	47.936922
1963.687326	160.542201	47.941927
1960.234653	161.192784	47.946932
1956.473298	160.878846	47.951937
1953.164877	162.804494	47.956941
1949.800266	165.627053	47.961946
1946.487753	161.394047	47.966951
1942.676475	166.246402	47.971956
1939.425658	160.122772	47.976961
1935.776797	164.751363	47.981965
1932.128715	159.768649	47.986970
1928.983222	155.375461	47.991975
1925.321998	162.431391	47.996980
1921.683083	153.099609	48.001985
1918.342576	160.489948	48.006989
1915.091899	158.620736	48.011994
1911.573259	156.662778	48.016999
1907.537014	164.130938	48.022004
1904.291358	160.817964	48.027009
1900.461728	155.581095	48.032013
1896.947256	153.717381	48.037018
1893.814475	153.957401	48.042023
1890.129682	154.075868	48.047028
1886.997770	153.760636	48.052033
1883.111552	160.945125	48.057037
1879.668725	155.099337	48.062042
1876.426863	152.325085	48.067047
1872.668002	151.671182	48.072052
1869.463191	153.441042	48.077057
1865.678979	161.751877	48.082061
1862.505834	159.446604	48.087066
1858.725954	160.754373	48.092071
1855.014134	166.255001	48.097076
1852.147800	153.185950	48.102081
1848.434522	152.393308	48.107085
1844.578076	163.674585	48.112090
1841.512221	154.224928	48.117095
1837.575534	157.055425	48.122100
1834.145503	150.815647	48.127105
1830.439907	154.116322	48.132109
1827.138161	155.453869	48.137114
1823.699918	147.023621	48.142119
1820.442656	157.127483	48.147124
1817.010313	150.679119	48.152129
1813.552623	156.349934	48.157133
1809.503164	150.947779	48.162138
1805.888216	155.806481	48.167143
1802.468258	165.065787	48.172148
1799.098997	160.624205	48.177153
1795.796843	161.214719	48.182157
1792.127771	154.413565	48.187162
1788.669450	154.446154	48.192167
1785.357913	160.366357	48.197172
1782.010499	153.079117	48.202177
1778.217652	158.912279	48.207181
1774.679613	148.919060	48.212186
1771.073619	157.018376	48.217191
1767.585322	154.965727	48.222196
1764.406731	147.132799	48.227201
1760.943887	154.014182	48.232205
1757.417436	150.835321	48.237210
1753.516452	147.032783	48.242215
1750.454095	151.343398	48.247220
1746.719951	153.076066	48.252225
1743.082201	150.643188	48.257229
1739.455267	156.333329	48.262234
1736.238421	150.605629	48.267239
1732.426719	160.947366	48.272244
1729.294778	150.263311	48.277249
1725.916544	153.290147	48.282253
1722.315522	157.124595	48.287258
1718.623358	149.267023	48.292263
1715.335974	153.214239	48.297268
1711.808484	151.210338	48.302273
1708.315078	151.290618	48.307277
1704.802777	145.979001	48.312282
1701.337803	154.025858	48.317287
1697.546159	154.578905	48.322292
1694.175580	142.420530	48.327297
1690.422625	150.218568	48.332301
1686.998502	155.966804	48.337306
1683.780913	156.819303	48.342311
1680.098308	160.282253	48.347316
1676.875239	144.820354	48.352321
1672.934588	153.540200	48.357325
1669.654630	145.729223	48.362330
1666.235338	145.775779	48.367335
1662.583562	147.321247	48.372340
1659.453085	144.687013	48.377345
1655.897820	140.172676	48.382349
1652.018899	155.040461	48.387354
1648.504363	147.078418	48.392359
1644.763012	150.593724	48.397364
1642.040386	137.873477	48.402369
1638.140962	144.659728	48.407373
1634.802747	143.273461	48.412378
1631.231680	144.178478	48.417383
1627.306675	148.305300	48.422388
1624.146096	148.436425	48.427393
1620.521106	137.425637	48.432397
1616.982667	145.880543	48.437402
1613.618963	142.058028	48.442407
1610.161377	146.249519	48.447412
1606.702690	143.582131	48.452417
1603.067132	149.957370	48.457421
1599.553802	152.689888	48.462426
1596.107143	147.825532	48.467431
1592.166151	151.444315	48.472436
1589.131621	140.527999	48.477441
1585.781137	143.293213	48.482445
1582.209159	143.491554	48.487450
1578.474810	137.051453	48.492455
1575.091864	138.413048	48.497460
1571.810976	136.684448	48.502465
1567.935475	135.458842	48.507469
1564.811751	136.810566	48.512474
1561.440779	140.426747	48.517479
1557.477260	138.169015	48.522484
1554.295179	139.874941	48.527489
1550.459225	140.472133	48.532493
1546.959480	139.598073	48.537498
1543.562149	135.658821	48.542503
1539.862316	149.777394	48.547508
1536.486752	143.886629	48.552513
1533.220816	139.540272	48.557517
1529.535941	139.817891	48.562522
1526.369371	127.709826	48.567527
1522.916466	140.824395	48.572532
1518.997090	138.276026	48.577537
1515.427148	143.587884	48.582541
1511.795450	144.343561	48.587546
1508.776087	139.888986	48.592551
1504.980062	144.018271	48.597556
1501.932709	133.636760	48.602561
1498.249100	138.842301	48.607565
1494.198004	149.623169	48.612570
1490.784341	141.272610	48.617575
1487.343369	148.291457	48.622580
1484.180443	137.906757	48.627585
1480.455107	146.455591	48.632589
1476.896366	143.077846	48.637594
1473.580265	136.488008	48.642599
1469.733586	148.112474	48.647604
1466.483962	139.408037	48.652609
1463.009321	141.345304	48.657613
1459.800882	144.697890	48.662618
1456.422796	141.510931	48.667623
1452.712732	137.170937	48.672628
1449.201853	129.166433	48.677633
1445.380871	149.724467	48.682637
1441.742535	140.559175	48.687642
1438.809625	142.173480	48.692647
1434.684972	144.350211	48.697652
1431.800180	139.723473	48.702657
1427.940125	141.589286	48.707661
1424.358967	135.124003	48.712666
1421.043072	136.895152	48.717671
1417.001708	132.933971	48.722676
1414.050022	133.001114	48.727681
1410.440355	150.257725	48.732685
1407.228794	148.401355	48.737690
1403.800213	140.666264	48.742695
1399.916905	149.477872	48.747700
1396.380752	140.255475	48.752705
1392.395691	144.916538	48.757709
1389.199098	142.853069	48.762714
1385.934483	133.296905	48.767719
1382.401609	139.895682	48.772724
1379.146296	140.427241	48.777729
1375.230089	140.303746	48.782733
1371.634483	148.140932	48.787738
1368.683807	138.143347	48.792743
1364.753710	139.441011	48.797748
1361.373191	134.510266	48.802753
1357.995695	136.769196	48.807757
1354.644674	134.919143	48.812762
1351.110223	132.358608	48.817767
1347.173341	149.190007	48.822772
1343.754162	140.136383	48.827777
1340.444006	149.872154	48.832781
1337.206556	143.328226	48.837786
1333.466237	140.210903	48.842791
1329.904903	141.177490	48.847796
1326.499236	133.724029	48.852801
1322.781525	149.175551	48.857805
1319.039184	135.329557	48.862810
1316.043976	141.633687	48.867815
1312.565970	148.718764	48.872820
1308.867134	136.570382	48.877825
1305.372100	137.791447	48.882829
1301.614272	145.387708	48.887834
1298.323897	145.644308	48.892839
1295.013532	148.673249	48.897844
1291.598882	135.715004	48.902849
1288.032530	144.578496	48.907853
1283.923491	133.323210	48.912858
1281.088101	140.208148	48.917863
1277.201886	145.525885	48.922868
1273.828258	139.333480	48.927873
1270.099131	146.289990	48.932877
1266.986890	134.877446	48.937882
1263.751676	126.796947	48.942887
1260.014491	140.004449	48.947892
1256.546853	138.657221	48.952897
1252.978455	145.561126	48.957901
1249.218238	144.115647	48.962906
1245.830124	138.142138	48.967911
1241.862294	141.308213	48.972916
1238.746614	134.968214	48.977921
1235.297643	136.699331	48.982925
1231.790556	145.645221	48.987930
1228.656492	136.931542	48.992935
1225.049064	138.886199	48.997940
1221.097185	138.857337	49.002945
1217.548833	143.811423	49.007949
1214.175539	131.499402	49.012954
1211.040904	125.005876	49.017959
1207.240215	134.411168	49.022964
1204.127808	130.221626	49.027969
1200.186449	144.155971	49.032973
1196.467936	131.965170	49.037978
1193.469658	137.416003	49.042983
1190.095874	137.797373	49.047988
1186.241461	133.155866	49.052993
1182.293689	137.374426	49.057997
1178.855561	140.897386	49.063002
1175.823367	142.121755	49.068007
1172.210382	140.440259	49.073012
1168.876340	144.755888	49.078017
1165.304488	142.170306	49.083021
1161.983724	144.738303	49.088026
1158.458094	143.988012	49.093031
1155.071773	134.371249	49.098036
1151.288137	137.515235	49.103041
1147.548621	143.014841	49.108045
1144.136012	142.420716	49.113050
1140.682627	144.360824	49.118055
1136.935044	143.763280	49.123060
1133.835013	146.726180	49.128065
1130.149946	141.365452	49.133069
1126.427265	142.774857	49.138074
1122.980917	138.512512	49.143079
1119.727367	133.950903	49.148084
1116.599183	140.947488	49.153089
1113.022416	135.579133	49.158093
1109.022648	134.604758	49.163098
1105.756676	124.568341	49.168103
1102.008286	135.875477	49.173108
1098.796788	134.349071	49.178113
1095.101996	130.111449	49.183117
1091.915781	133.155522	49.188122
1088.419273	128.971752	49.193127
1084.056866	131.146857	49.198132
1081.100717	139.218129	49.203137
1077.531631	139.936167	49.208141
1073.820525	132.309836	49.213146
1070.923374	136.857389	49.218151
1067.327580	133.900119	49.223156
1063.940855	128.333637	49.228161
1060.421032	128.481529	49.233165
1057.056976	128.635241	49.238170
1053.354068	130.617460	49.243175
1049.550318	137.456031	49.248180
1046.247594	122.878125	49.253185
1042.694591	130.589495	49.258189
1038.538895	129.971899	49.263194
1035.414267	128.519977	49.268199
1032.026925	131.322062	49.273204
1028.942423	132.657595	49.278209
1025.379797	133.294092	49.283213
1021.667942	139.386951	49.288218
1018.100590	127.878384	49.293223
1014.535545	136.447418	49.298228
1011.292799	128.414147	49.303233
1007.387456	136.264518	49.308237
1003.837019	136.446722	49.313242
1000.567586	138.772697	49.318247
996.840207	135.587219	49.323252
993.903930	128.364065	49.328257
990.129067	135.228293	49.333261
986.885951	135.665365	49.338266
982.942091	127.808046	49.343271
979.246025	132.214257	49.348276
976.174660	125.964616	49.353281
972.617865	130.783914	49.358285
968.659608	129.235656	49.363290
965.950977	122.371723	49.368295
962.181637	124.823609	49.373300
958.531934	128.325670	49.378305
954.996970	124.545017	49.383309
951.450988	130.175369	49.388314
948.221846	126.421502	49.393319
944.443863	136.114700	49.398324
941.130104	135.614300	49.403329
937.578484	132.536562	49.408333
933.960392	131.325174	49.413338
930.584329	130.904548	49.418343
926.527113	127.632782	49.423348
923.542348	127.299991	49.428353
919.812884	129.978569	49.433357
916.779430	124.878895	49.438362
913.192082	119.816561	49.443367
909.575067	127.689573	49.448372
906.199391	125.222726	49.453377
902.449340	117.728109	49.458381
899.055830	114.300431	49.463386
895.761291	116.006654	49.468391
891.971350	114.039511	49.473396
888.495507	112.160533	49.478401
884.833417	115.059469	49.483405
881.411188	121.774680	49.488410
877.992767	123.624148	49.493415
874.345288	129.447367	49.498420
870.870831	111.221466	49.503425
867.745678	116.586123	49.508429
864.120533	121.007529	49.513434
860.753607	120.815145	49.518439
856.976677	126.772267	49.523444
853.443979	113.011661	49.528449
849.944763	123.133407	49.533453
846.280952	126.644006	49.538458
843.013549	118.916682	49.543463
839.507774	118.256504	49.548468
835.810768	121.335503	49.553473
832.412914	114.236968	49.558477
829.079393	114.763107	49.563482
825.399861	115.781406	49.568487
821.731818	124.230853	49.573492
818.558531	117.958922	49.578497
814.725623	115.870093	49.583501
811.222947	129.189674	49.588506
808.109443	115.780097	49.593511
804.271349	130.242087	49.598516
801.026660	122.513801	49.603521
797.737715	111.945289	49.608525
793.741847	121.813357	49.613530
790.044315	118.801911	49.618535
786.709753	116.988644	49.623540
784.012188	112.855909	49.628545
779.731480	114.829530	49.633549
776.314149	112.084922	49.638554
772.815440	109.800348	49.643559
769.273575	117.157032	49.648564
766.066838	115.501620	49.653569
762.258553	119.090055	49.658573
758.747162	116.706553	49.663578
755.765663	115.581231	49.668583
751.721616	119.977886	49.673588
748.561212	117.933965	49.678593
745.016112	113.923100	49.683597
741.602265	114.150013	49.688602
737.858727	113.191804	49.693607
734.009452	118.999567	49.698612
730.938581	110.152510	49.703617
727.170683	108.261195	49.708621
723.739492	121.333974	49.713626
720.965880	113.234986	49.718631
716.953591	105.067008	49.723636
712.884189	105.759959	49.728641
709.554808	110.678582	49.733645
706.090040	118.673764	49.738650
702.795457	103.633863	49.743655
699.336520	122.089029	49.748660
695.741844	108.558267	49.753665
692.540748	114.998250	49.758669
688.740728	106.401895	49.763674
685.601694	112.688745	49.768679
681.598282	115.562611	49.773684
678.377509	111.304564	49.778689
674.921602	107.452857	49.783693
671.539969	114.037767	49.788698
668.111285	110.047768	49.793703
664.150246	113.167820	49.798708
660.646726	104.413710	49.803713
657.121180	109.890720	49.808717
653.715662	116.619309	49.813722
650.218046	106.134192	49.818727
646.747323	109.057898	49.823732
643.639025	105.522462	49.828737
639.731005	101.161472	49.833741
635.990107	109.136275	49.838746
632.621856	99.957842	49.843751
629.199757	114.092808	49.848756
626.021827	111.336143	49.853761
622.342171	113.400507	49.858765
618.562527	120.352439	49.863770
615.307130	116.280531	49.868775
611.399767	113.975293	49.873780
608.245115	114.443194	49.878785
604.653950	117.687993	49.883789
601.074376	130.099471	49.888794
597.726897	115.165692	49.893799
594.457122	120.163534	49.898804
590.711776	112.622058	49.903809
587.203287	112.516452	49.908813
583.401948	115.498263	49.913818
580.368066	108.021028	49.918823
576.991765	117.163375	49.923828
573.250590	116.859083	49.928833
569.590804	112.471094	49.933837
566.163913	116.824406	49.938842
563.018693	115.306771	49.943847
559.264872	112.176970	49.948852
555.892367	104.967524	49.953857
552.428419	112.338505	49.958861
548.633684	117.687471	49.963866
545.024772	112.821626	49.968871
541.242440	116.293270	49.973876
538.136806	115.107928	49.978881
534.582795	110.575385	49.983885
531.141470	112.040153	49.988890
527.773784	104.608919	49.993895
524.070756	118.632571	49.998900
520.768509	115.793349	50.003905
517.027791	108.939088	50.008909
513.549750	123.453197	50.013914
510.436023	109.801984	50.018919
506.944766	103.994956	50.023924
503.247229	109.409963	50.028929
499.659246	107.599191	50.033933
495.972457	114.591106	50.038938
492.710486	102.816434	50.043943
488.545606	121.839449	50.048948
485.683722	110.730093	50.053953
482.203763	115.162500	50.058957
478.872644	121.868247	50.063962
475.627803	112.826994	50.068967
471.490709	116.648076	50.073972
468.182662	109.377518	50.078977
464.800069	111.651361	50.083981
460.822014	115.854618	50.088986
457.336884	113.658830	50.093991
453.935442	118.699871	50.098996
450.672857	114.346503	50.104001
447.006419	114.351805	50.109005
443.351206	123.099950	50.114010
440.355772	110.109040	50.119015
436.288736	124.396844	50.124020
433.155056	111.213130	50.129025
429.410439	120.350621	50.134029
426.041068	122.001886	50.139034
422.766278	109.229890	50.144039
418.979115	118.784095	50.149044
415.644159	111.846399	50.154049
412.054855	112.710001	50.159053
408.371454	115.476093	50.164058
404.987622	110.031637	50.169063
401.152444	112.046538	50.174068
397.751753	109.299089	50.179073
394.573238	109.060294	50.184077
390.937600	109.687873	50.189082
387.576116	110.457353	50.194087
384.083816	110.317264	50.199092
380.751780	111.509698	50.204097
377.367080	109.324983	50.209101
373.287821	111.390960	50.214106
370.077185	115.988251	50.219111
366.597786	123.740811	50.224116
363.035722	111.460217	50.229121
359.758086	122.912566	50.234125
355.736040	117.538847	50.239130
352.471496	105.682828	50.244135
348.802800	122.362573	50.249140
345.647634	119.494410	50.254145
342.108263	115.277121	50.259149
338.332322	105.546590	50.264154
335.057943	107.012493	50.269159
331.361200	116.000052	50.274164
328.011430	109.269322	50.279169
324.597650	111.895347	50.284173
320.768208	108.094316	50.289178
317.249653	101.287539	50.294183
313.758292	111.494386	50.299188
310.618821	106.471723	50.304193
306.821392	106.499614	50.309197
303.536846	105.553232	50.314202
299.970729	108.121610	50.319207
296.426764	107.488914	50.324212
292.859276	106.276598	50.329217
289.398200	103.038202	50.334221
285.835495	109.364456	50.339226
282.598533	103.508033	50.344231
279.012417	111.110778	50.349236
275.557786	103.170230	50.354241
271.961095	107.974950	50.359245
268.354951	104.971929	50.364250
264.899370	106.638572	50.369255
261.015974	116.355447	50.374260
257.824906	114.163049	50.379265
254.614723	105.819946	50.384269
250.955061	121.572762	50.389274
247.305931	111.083295	50.394279
243.765058	108.376542	50.399284
240.346502	110.699133	50.404289
236.962422	106.489385	50.409293
233.139942	111.106353	50.414298
229.588382	104.397272	50.419303
226.067984	111.541822	50.424308
223.120661	112.043959	50.429313
219.175275	113.606817	50.434317
215.634262	117.275391	50.439322
212.727344	115.061051	50.444327
208.706951	109.853561	50.449332
205.542371	98.442103	50.454337
202.202381	109.739302	50.459341
198.067221	99.953332	50.464346
194.917053	105.557792	50.469351
191.363036	110.174162	50.474356
187.584585	106.410201	50.479361
184.549793	106.724379	50.484365
180.710132	103.639522	50.489370
177.644541	106.339837	50.494375
174.134262	108.088029	50.499380
170.347975	106.379235	50.504385
166.760232	104.012619	50.509389
162.846081	100.686931	50.514394
159.763729	107.037162	50.519399
156.352187	105.915966	50.524404
152.834097	117.284719	50.529409
149.678884	105.889513	50.534413
145.788063	118.021897	50.539418
142.236145	99.259984	50.544423
138.579287	117.118555	50.549428
134.861069	108.455124	50.554433
131.725333	109.788114	50.559437
128.335864	117.167203	50.564442
125.197938	112.567117	50.569447
121.467837	109.880352	50.574452
117.892780	107.601662	50.579457
113.789968	110.584056	50.584461
110.817274	109.775238	50.589466
107.584781	106.494217	50.594471
103.505981	107.525747	50.599476
100.136877	106.003691	50.604481
97.153103	100.282512	50.609485
93.171554	110.373536	50.614490
89.989259	104.761399	50.619495
86.255870	107.427106	50.624500
82.634626	107.190804	50.629505
79.196317	105.806715	50.634509
75.169497	110.636632	50.639514
72.133635	102.339809	50.644519
68.438187	113.969261	50.649524
65.502652	104.414798	50.654529
61.975847	114.565928	50.659533
58.352937	109.006839	50.664538
54.904728	106.745484	50.669543
51.068204	106.376923	50.674548
47.451509	107.417438	50.679553
44.356736	107.622458	50.684557
40.471342	113.897549	50.689562
37.264462	110.915052	50.694567
33.912861	108.355530	50.699572
30.232174	100.156633	50.704577
26.787002	110.139559	50.709581
22.816428	102.902916	50.714586
19.816295	97.182335	50.719591
15.928497	100.920326	50.724596
12.155632	103.225986	50.729601
9.247568	101.145577	50.734605
6.012655	108.296693	50.739610
2.371522	99.885849	50.744615