Tue Jun 21 11:13:31 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.797955	123.208358	0.000000
0.784727	132.439907	0.005005
0.876629	108.910207	0.010010
0.090163	92.838389	0.015014
0.133205	94.452991	0.020019
0.270574	96.288379	0.025024
0.388540	89.500339	0.030029
0.206671	78.514152	0.035034
0.068896	76.122434	0.040038
-0.095768	67.184885	0.045043
-0.362044	52.453493	0.050048
-0.912161	43.799022	0.055053
-1.165779	28.741141	0.060058
-1.612011	25.638213	0.065062
-1.869783	5.372246	0.070067
-1.950776	-1.575601	0.075072
-2.030348	-0.453178	0.080077
-2.014995	-17.911702	0.085082
-2.943208	-5.781856	0.090086
-3.914264	-10.523542	0.095091
-4.205403	-10.259804	0.100096
-4.848286	-4.541370	0.105101
-4.332518	-6.697740	0.110106
-4.809054	-3.491464	0.115110
-4.579787	-5.436409	0.120115
-5.064393	-2.461846	0.125120
-5.029848	4.357219	0.130125
-5.170183	-6.928232	0.135130
-5.853015	-0.100092	0.140134
-6.390876	-3.972830	0.145139
-6.361858	-4.435603	0.150144
-6.625308	-3.944978	0.155149
-6.425261	-10.821749	0.160154
-6.592523	-0.796164	0.165158
-7.444525	3.248989	0.170163
-7.906828	-0.718943	0.175168
-8.456160	-6.051816	0.180173
-8.064153	-3.778300	0.185178
-8.512734	4.053558	0.190182
-8.468302	1.323053	0.195187
-8.196786	-4.577906	0.200192
-8.727222	5.231754	0.205197
-9.273014	-2.266050	0.210202
-9.324419	-4.197669	0.215206
-9.600693	2.310365	0.220211
-9.707680	0.887200	0.225216
-10.687418	-3.738793	0.230221
-11.145009	-7.805182	0.235226
-11.257581	4.985646	0.240230
-11.374597	-3.603960	0.245235
-11.154725	-7.621116	0.250240
-11.263400	-2.332133	0.255245
-11.293486	-11.644751	0.260250
-12.183751	-4.860013	0.265254
-12.865280	0.993879	0.270259
-13.041691	-3.224449	0.275264
-13.043645	-0.210226	0.280269
-12.843660	-6.685219	0.285274
-13.393663	-3.947676	0.290278
-13.019963	0.807762	0.295283
-13.262863	2.764914	0.300288
-14.238080	-5.486232	0.305293
-14.448212	-9.086257	0.310298
-14.636969	-2.583048	0.315302
-14.667932	0.295873	0.320307
-14.327200	-11.133369	0.325312
-15.435898	-4.665289	0.330317
-15.806394	-8.089772	0.335322
-16.124922	-6.230604	0.340326
-16.233248	-7.216060	0.345331
-16.054247	-6.821989	0.350336
-16.426856	-10.877388	0.355341
-17.200853	-7.380318	0.360346
-17.487259	-4.988739	0.365350
-17.980969	-3.498580	0.370355
-17.866440	-2.861177	0.375360
-17.772363	0.968900	0.380365
-17.473853	-8.474304	0.385370
-17.605986	0.414355	0.390374
-18.216921	-8.650329	0.395379
-18.815065	-4.188417	0.400384
-19.502950	-0.164125	0.405389
-19.342680	1.130911	0.410394
-19.463586	0.678954	0.415398
-19.675191	4.751064	0.420403
-20.363809	-3.526623	0.425408
-21.031595	-3.750280	0.430413
-20.694165	-6.042880	0.435418
-20.863303	-1.780669	0.440422
-20.690666	-3.571000	0.445427
-20.607313	-2.981517	0.450432
-21.537258	3.619964	0.455437
-21.956168	-10.131394	0.460442
-22.273484	-2.104605	0.465446
-22.336344	-4.565349	0.470451
-22.242284	-9.018692	0.475456
-22.693013	5.318388	0.480461
-23.375849	-3.075696	0.485466
-23.460261	-0.035189	0.490470
-24.289413	2.421603	0.495475
-24.070599	-6.405751	0.500480
-24.477512	0.650201	0.505485
-24.282342	-1.743950	0.510490
-24.098142	-1.572147	0.515494
-24.553480	4.102014	0.520499
-24.855927	-0.169640	0.525504
-25.779617	3.377481	0.530509
-25.428102	4.009186	0.535514
-25.944782	1.362719	0.540518
-26.091680	2.284357	0.545523
-26.033783	0.869408	0.550528
-27.003851	5.693254	0.555533
-27.100714	-8.816897	0.560538
-27.309900	-3.603622	0.565542
-27.553866	2.555901	0.570547
-27.298965	-5.370095	0.575552
-27.740728	-2.362171	0.580557
-27.520310	4.263312	0.585562
-27.991184	6.975718	0.590566
-28.403960	0.887735	0.595571
-28.407696	-1.065789	0.600576
-29.239976	11.278671	0.605581
-29.720654	-0.855585	0.610586
-29.802050	-4.296566	0.615590
-29.914913	3.841013	0.620595
-30.422370	-2.536563	0.625600
-30.831027	8.463371	0.630605
-30.089424	-1.843530	0.635610
-30.312378	-0.681181	0.640614
-31.205349	-0.826501	0.645619
-31.366483	-3.564009	0.650624
-31.677465	1.920289	0.655629
-31.733417	-3.654912	0.660634
-31.895345	9.825875	0.665638
-32.390869	-3.121693	0.670643
-33.080631	-5.435405	0.675648
-33.834370	-4.404987	0.680653
-33.367176	-4.654782	0.685658
-33.599594	11.492392	0.690662
-33.523043	0.655278	0.695667
-33.417583	-7.342662	0.700672
-33.866953	2.103505	0.705677
-33.645533	2.406488	0.710682
-34.470137	5.076240	0.715686
-34.921051	-0.702324	0.720691
-34.852115	-0.640094	0.725696
-35.289157	9.619808	0.730701
-36.283935	1.492870	0.735706
-36.361099	10.810509	0.740710
-36.694517	3.345422	0.745715
-36.216589	8.860694	0.750720
-36.680843	5.413651	0.755725
-36.500930	2.156328	0.760730
-36.810353	10.723494	0.765734
-37.243679	8.971941	0.770739
-37.756597	-4.749444	0.775744
-38.065721	7.199553	0.780749
-38.114822	2.428332	0.785754
-38.265568	2.809522	0.790758
-38.303692	0.252922	0.795763
-38.422217	-5.063870	0.800768
-39.512811	6.476611	0.805773
-39.628651	2.843408	0.810778
-39.482467	10.119359	0.815782
-39.779929	1.849122	0.820787
-39.771497	-0.331573	0.825792
-40.461318	4.518090	0.830797
-40.790811	9.005375	0.835802
-41.391205	6.777107	0.840806
-41.515972	-1.855218	0.845811
-41.288913	6.178908	0.850816
-41.405680	1.397383	0.855821
-41.506242	-0.466303	0.860826
-42.147774	1.183116	0.865830
-42.778193	-3.778560	0.870835
-42.763278	1.784772	0.875840
-43.083988	0.637747	0.880845
-43.056438	-2.080885	0.885850
-42.958156	8.453063	0.890854
-43.437083	3.309024	0.895859
-43.924439	2.632804	0.900864
-44.397806	7.594425	0.905869
-44.380582	5.508177	0.910874
-44.748213	1.991461	0.915878
-44.606230	13.708879	0.920883
-44.921198	-1.883046	0.925888
-45.933666	1.229059	0.930893
-46.020012	6.257024	0.935898
-46.306529	4.419593	0.940902
-46.616461	7.396611	0.945907
-46.254623	-5.124812	0.950912
-46.560498	2.565014	0.955917
-46.290205	5.134159	0.960922
-46.688173	7.980914	0.965926
-47.556778	14.169884	0.970931
-47.626668	-2.219594	0.975936
-47.780756	3.875515	0.980941
-48.090727	-6.500550	0.985946
-48.075408	-2.827337	0.990950
-49.004795	2.198553	0.995955
-49.507707	2.437179	1.000960
-49.769446	-0.521059	1.005965
-49.521167	2.176050	1.010970
-49.322396	-1.883591	1.015974
-49.683803	-1.079954	1.020979
-49.406289	-0.197028	1.025984
-50.467247	13.500328	1.030989
-50.681042	2.423981	1.035994
-51.049466	4.921301	1.040998
-51.060306	15.967444	1.046003
-50.995191	13.185362	1.051008
-51.971492	12.020218	1.056013
-52.360254	10.200903	1.061018
-52.890908	0.106073	1.066022
-52.949639	8.655007	1.071027
-52.314634	0.010326	1.076032
-52.486750	3.723264	1.081037
-52.783417	2.268563	1.086042
-52.927866	7.820400	1.091046
-53.782364	3.223405	1.096051
-53.949627	4.055866	1.101056
-53.791257	6.583952	1.106061
-54.298278	5.724906	1.111066
-54.290332	0.764469	1.116070
-55.497313	2.592779	1.121075
-55.445830	7.686127	1.126080
-55.823418	4.599075	1.131085
-56.064343	4.615926	1.136090
-55.929628	13.275498	1.141094
-55.884033	18.985502	1.146099
-55.657081	6.071813	1.151104
-57.014805	13.052773	1.156109
-57.383400	8.482855	1.161114
-57.048441	-1.034665	1.166118
-57.548432	4.717339	1.171123
-57.376564	4.354439	1.176128
-57.515205	1.110799	1.181133
-58.490545	0.144015	1.186138
-58.726029	3.738983	1.191142
-59.246068	12.726222	1.196147
-59.166748	0.871600	1.201152
-59.226840	3.182488	1.206157
-59.232976	0.395238	1.211162
-58.907294	-1.141609	1.216166
-59.548511	8.117096	1.221171
-60.024894	3.661921	1.226176
-60.451019	12.488567	1.231181
-60.515844	5.682690	1.236186
-60.797777	10.670231	1.241190
-61.612059	15.786190	1.246195
-62.105436	2.913848	1.251200
-62.302929	5.806337	1.256205
-61.619985	6.236534	1.261210
-61.825328	5.051856	1.266214
-62.317285	11.428471	1.271219
-62.382590	13.334706	1.276224
-63.121293	17.011632	1.281229
-63.541755	9.286274	1.286234
-64.115683	13.710837	1.291238
-64.130431	8.323380	1.296243
-63.593946	-0.585395	1.301248
-63.918219	8.516828	1.306253
-63.979067	1.755286	1.311258
-64.293546	6.558777	1.316262
-64.817718	3.309127	1.321267
-65.054628	2.371212	1.326272
-65.512564	7.037437	1.331277
-65.434226	3.374447	1.336282
-66.080392	4.518874	1.341286
-66.387213	4.752061	1.346291
-66.711018	5.169608	1.351296
-66.731009	4.532023	1.356301
-66.638911	4.292248	1.361306
-66.870137	3.689251	1.366310
-67.433777	7.873731	1.371315
-68.073227	8.434126	1.376320
-68.596114	6.128895	1.381325
-68.374503	3.519020	1.386330
-68.594199	9.083120	1.391334
-69.112663	2.952854	1.396339
-68.734645	0.338784	1.401344
-69.144665	7.474188	1.406349
-68.702736	-1.911469	1.411354
-69.455069	10.963009	1.416358
-70.234747	2.674955	1.421363
-70.127641	2.688437	1.426368
-70.549480	9.850860	1.431373
-70.015950	4.751089	1.436378
-71.130461	3.653831	1.441382
-71.732042	6.580286	1.446387
-71.543687	6.766002	1.451392
-71.864281	4.568757	1.456397
-71.709299	-6.320804	1.461402
-72.084191	1.575021	1.466406
-72.617884	7.996040	1.471411
-73.098123	3.052122	1.476416
-73.335017	6.578455	1.481421
-73.542636	-3.590783	1.486426
-73.363814	3.050858	1.491430
-73.920742	4.124465	1.496435
-73.515943	3.072582	1.501440
-73.699536	6.640803	1.506445
-74.508609	2.043197	1.511450
-75.188962	-1.809483	1.516454
-75.275009	7.579872	1.521459
-75.156509	0.543543	1.526464
-75.258436	16.747645	1.531469
-75.278317	-1.300797	1.536474
-75.857826	3.016550	1.541478
-76.682834	6.929571	1.546483
-76.573840	0.244884	1.551488
-77.088641	14.790702	1.556493
-76.737200	7.386641	1.561498
-76.543633	4.137712	1.566502
-77.484599	4.588993	1.571507
-77.972989	-2.035832	1.576512
-78.360069	2.629906	1.581517
-78.610612	-0.616907	1.586522
-78.590580	6.129767	1.591526
-78.509779	0.003661	1.596531
-78.586770	-6.880903	1.601536
-78.994627	10.426033	1.606541
-79.483065	3.242171	1.611546
-79.368728	-3.877728	1.616550
-79.861751	5.786816	1.621555
-79.601020	-3.744457	1.626560
-80.589680	5.126014	1.631565
-81.235115	1.736611	1.636570
-81.381786	5.581692	1.641574
-81.641368	3.901616	1.646579
-81.277705	7.027164	1.651584
-81.616168	-0.641120	1.656589
-81.627659	-1.699838	1.661594
-82.192198	-0.869069	1.666598
-82.828232	6.735528	1.671603
-82.915461	0.674940	1.676608
-83.258029	5.618058	1.681613
-83.229075	-0.833939	1.686618
-83.108312	5.299319	1.691622
-83.746139	5.088865	1.696627
-84.374063	1.691826	1.701632
-84.829196	1.233261	1.706637
-84.508599	-6.085962	1.711642
-84.701767	-2.681917	1.716646
-84.742379	10.045684	1.721651
-84.605386	3.401350	1.726656
-85.420861	10.819983	1.731661
-85.992056	7.063481	1.736666
-86.478533	6.520320	1.741670
-86.500081	8.565334	1.746675
-85.743246	3.871788	1.751680
-86.492527	5.209513	1.756685
-86.992371	3.844506	1.761690
-87.539218	3.123484	1.766694
-87.885956	8.330732	1.771699
-87.877557	4.599997	1.776704
-88.172787	7.130189	1.781709
-88.152376	2.762844	1.786714
-88.393925	-2.911264	1.791718
-88.503805	2.041466	1.796723
-89.268041	6.257393	1.801728
-89.365902	7.051722	1.806733
-89.783095	9.163641	1.811738
-89.424497	13.868491	1.816742
-89.458476	14.310856	1.821747
-90.057432	6.974013	1.826752
-90.943908	12.156987	1.831757
-90.985999	13.394366	1.836762
-91.357249	1.784863	1.841766
-91.184710	9.614696	1.846771
-90.991750	-2.639986	1.851776
-91.516324	2.189221	1.856781
-92.175432	-1.175419	1.861786
-92.702582	0.219054	1.866790
-92.692139	8.080271	1.871795
-92.569246	-9.461768	1.876800
-92.822292	2.613107	1.881805
-92.811231	7.621388	1.886810
-93.245948	4.684500	1.891814
-94.100856	8.046195	1.896819
-93.946492	-0.658993	1.901824
-94.512362	-5.732381	1.906829
-94.148384	7.729774	1.911834
-95.185102	-0.506230	1.916838
-95.688839	-0.723497	1.921843
-95.221594	-3.545534	1.926848
-95.569879	-1.717741	1.931853
-95.574148	2.248991	1.936858
-95.769101	-7.908525	1.941862
-95.928938	-2.937262	1.946867
-96.345270	-11.685863	1.951872
-97.141439	-0.544011	1.956877
-97.155100	-6.295521	1.961882
-97.255919	-11.870191	1.966886
-97.790514	-8.432294	1.971891
-97.479130	-12.685025	1.976896
-97.995911	5.274760	1.981901
-98.403329	-5.156987	1.986906
-98.695701	-2.777044	1.991910
-99.108310	-6.938486	1.996915
-99.247924	-5.535960	2.006912
-98.445011	-8.916754	2.016909
-97.903518	-1.155908	2.026906
-97.837698	1.535839	2.036902
-97.790087	0.163119	2.046899
-96.542056	-0.754798	2.056896
-96.213065	-4.174272	2.066893
-96.070933	2.474517	2.076890
-95.090717	-1.905389	2.086886
-94.926836	0.248099	2.096883
-94.196754	1.735018	2.106880
-93.386834	3.761557	2.116877
-93.389450	-1.441526	2.126874
-92.949429	-4.577281	2.136870
-92.275660	-1.206350	2.146867
-91.997240	-2.170556	2.156864
-91.205402	2.329581	2.166861
-90.659676	3.392981	2.176858
-90.518144	0.725541	2.186854
-89.649078	1.092845	2.196851
-89.169274	1.644947	2.206848
-88.925779	3.085997	2.216845
-87.993994	-5.229682	2.226842
-87.806620	-2.529415	2.236838
-87.479743	0.156837	2.246835
-86.349715	-5.071213	2.256832
-85.790226	-8.208969	2.266829
-85.987579	-5.496557	2.276826
-85.758166	-2.856798	2.286822
-84.715679	-1.093032	2.296819
-84.342013	-4.698718	2.306816
-83.249847	-3.049678	2.316813
-82.644791	-0.711207	2.326810
-82.752008	9.638748	2.336806
-82.753140	3.465273	2.346803
-82.025382	5.676531	2.356800
-81.340980	2.275650	2.366797
-80.413227	-4.344871	2.376794
-80.382897	-9.584232	2.386790
-80.047092	-11.450037	2.396787
-78.999637	-5.648063	2.406784
-78.563362	-3.370355	2.416781
-78.271838	-8.806101	2.426778
-77.346208	-6.428646	2.436774
-77.398384	0.463146	2.446771
-76.969005	2.323314	2.456768
-76.007441	-5.606077	2.466765
-75.451812	-1.245040	2.476762
-75.390051	3.132979	2.486758
-74.837126	2.639602	2.496755
-73.977755	3.428779	2.506752
-73.865806	2.436227	2.516749
-73.322990	2.236951	2.526746
-72.849940	1.260666	2.536742
-72.228331	3.520131	2.546739
-71.041759	1.672685	2.556736
-70.998201	-5.060439	2.566733
-70.867315	-2.444471	2.576730
-70.570484	-2.469838	2.586726
-69.617436	-1.917864	2.596723
-69.419302	-2.058279	2.606720
-68.250454	-6.441360	2.616717
-67.987059	-5.366766	2.626714
-67.761440	-6.216716	2.636710
-67.602223	-2.391675	2.646707
-66.689631	-5.114690	2.656704
-66.392949	-0.426641	2.666701
-65.148183	-8.198429	2.676698
-64.861597	-7.396983	2.686694
-64.705479	-7.827213	2.696691
-64.359120	-0.051827	2.706688
-64.120881	1.090754	2.716685
-63.160274	-0.160498	2.726682
-62.456372	-3.889434	2.736678
-61.759345	-4.552688	2.746675
-61.401482	-6.843198	2.756672
-61.337284	-7.748611	2.766669
-61.022263	-5.248889	2.776666
-60.239363	0.860879	2.786662
-59.763204	-0.933130	2.796659
-58.795021	-1.473342	2.806656
-58.174372	0.079522	2.816653
-57.824609	3.996697	2.826650
-57.814148	3.283147	2.836646
-57.757733	2.339110	2.846643
-56.701572	3.155373	2.856640
-56.431840	1.371641	2.866637
-55.347660	-3.153904	2.876634
-55.069324	1.856680	2.886630
-54.980335	-0.788623	2.896627
-54.199997	4.449827	2.906624
-53.793045	4.560737	2.916621
-53.080314	-4.170539	2.926618
-52.350372	2.599835	2.936614
-52.107492	-1.983774	2.946611
-51.874733	-2.105620	2.956608
-50.941398	-2.226710	2.966605
-50.444579	-2.343284	2.976602
-50.386344	0.675342	2.986598
-49.612446	-2.845865	2.996595
-48.935200	4.154532	3.006592
-48.795475	-2.758515	3.016589
-48.260430	-2.894855	3.026586
-47.458596	5.320410	3.036582
-47.218390	-0.957641	3.046579
-46.414369	-0.205330	3.056576
-45.752196	-2.009791	3.066573
-45.626353	0.600494	3.076570
-45.405794	-5.011603	3.086566
-44.693297	0.737380	3.096563
-44.160143	1.566953	3.106560
-43.615668	4.436891	3.116557
-42.830695	2.730447	3.126554
-42.371114	-0.416842	3.136550
-42.174239	3.957575	3.146547
-42.121176	4.901624	3.156544
-41.124946	6.476663	3.166541
-40.787306	0.669523	3.176538
-39.609648	-2.050555	3.186534
-39.238967	3.495211	3.196531
-39.295194	6.592860	3.206528
-38.955730	-2.612651	3.216525
-37.997775	-2.826927	3.226522
-37.846894	-0.722655	3.236518
-36.877852	-1.735430	3.246515
-36.213888	-1.399154	3.256512
-36.100326	-5.758822	3.266509
-35.805316	-5.491458	3.276506
-35.324264	-2.440304	3.286502
-34.538841	-0.930926	3.296499
-34.369715	2.319876	3.306496
-32.885687	-2.659937	3.316493
-32.750568	-2.894437	3.326490
-33.003874	-2.498139	3.336486
-32.275441	-1.304547	3.346483
-31.162924	1.366012	3.356480
-30.913138	-2.119575	3.366477
-30.785646	-1.032549	3.376474
-30.647470	-3.976249	3.386470
-29.827766	2.558760	3.396467
-28.895350	2.734599	3.406464
-28.486881	3.838324	3.416461
-28.280990	3.212542	3.426458
-27.447337	7.183356	3.436454
-27.076184	9.175478	3.446451
-27.050371	6.953588	3.456448
-25.496674	2.386652	3.466445
-25.257427	2.086105	3.476442
-24.893910	5.099031	3.486438
-25.055232	-0.185657	3.496435
-24.296396	0.095985	3.506432
-23.551730	3.939867	3.516429
-23.066004	5.718987	3.526426
-22.238858	9.032724	3.536422
-22.175139	4.397179	3.546419
-21.814153	4.217350	3.556416
-20.710311	3.184232	3.566413
-20.396706	2.826322	3.576410
-20.295717	-0.379740	3.586406
-19.490017	6.978560	3.596403
-18.832301	6.008254	3.606400
-18.767703	3.241720	3.616397
-18.098524	-1.338586	3.626394
-17.553230	1.377301	3.636390
-17.243460	4.920160	3.646387
-15.912501	10.408473	3.656384
-15.918840	1.244219	3.666381
-15.946193	0.567754	3.676378
-15.391490	1.193213	3.686374
-14.449624	0.925887	3.696371
-14.175683	1.503591	3.706368
-13.234291	1.324665	3.716365
-12.282962	-0.785523	3.726362
-12.783101	0.881024	3.736358
-12.429238	4.485934	3.746355
-11.741670	-0.086746	3.756352
-10.969211	-2.760267	3.766349
-10.681016	-0.418710	3.776346
-9.214011	-1.365552	3.786342
-9.402755	1.924359	3.796339
-9.149363	9.336383	3.806336
-8.831116	5.817131	3.816333
-7.777546	-9.130891	3.826330
-7.449873	1.222923	3.836326
-7.470511	3.486006	3.846323
-6.340070	-5.398607	3.856320
-5.472359	3.757528	3.866317
-5.580328	-1.459531	3.876314
-5.400531	-7.932868	3.886310
-4.624710	-0.621783	3.896307
-4.290291	-1.759648	3.906304
-3.520305	5.442747	3.916301
-3.258299	11.333916	3.926298
-2.673562	18.342536	3.936294
-2.207943	28.284876	3.946291
-1.898244	37.735960	3.956288
-1.488662	49.089463	3.966285
-1.073304	69.287350	3.976282
-0.529734	82.056524	3.986278
-0.248779	110.110819	3.996275
0.000000	126.542040	4.001280
0.003064	137.928349	4.006285
0.394530	151.914956	4.011290
0.574298	167.148660	4.016294
0.390483	177.002855	4.021299
0.711219	186.648791	4.026304
1.249300	198.635643	4.031309
1.019189	198.119079	4.036314
0.914211	196.516383	4.041318
0.742158	193.981533	4.046323
1.447933	206.854481	4.051328
1.088986	200.891490	4.056333
1.411744	203.002653	4.061338
1.021562	214.971746	4.066342
1.082431	216.415082	4.071347
1.482266	231.463420	4.076352
1.414978	225.154739	4.081357
1.777703	229.014981	4.086362
1.733438	222.649603	4.091366
1.604831	206.364734	4.096371
1.308144	211.186849	4.101376
1.300141	198.443721	4.106381
1.363099	196.722047	4.111386
0.815509	207.875764	4.116390
1.534214	212.022785	4.121395
1.511815	224.926343	4.126400
1.430368	232.081834	4.131405
1.616159	229.884761	4.136410
1.234411	223.961057	4.141414
1.322009	228.997984	4.146419
1.618510	232.233378	4.151424
1.220643	240.188184	4.156429
1.388001	232.052390	4.161434
1.565042	235.444911	4.166438
1.451128	233.642803	4.171443
1.468803	237.587219	4.176448
1.476255	235.615433	4.181453
1.552206	234.017701	4.186458
1.507194	231.979221	4.191462
1.610448	234.383273	4.196467
1.249099	239.407520	4.201472
1.432785	247.748515	4.206477
1.802550	249.569316	4.211482
1.768676	269.315454	4.216486
1.712716	260.539368	4.221491
1.948655	265.433341	4.226496
2.007284	248.864833	4.231501
1.568650	236.792686	4.236506
1.371957	238.679067	4.241510
1.701070	249.055770	4.246515
1.644256	257.869155	4.251520
1.882993	264.275046	4.256525
2.261870	264.752259	4.261530
2.056360	263.702956	4.266534
2.072339	253.283783	4.271539
1.846783	237.875517	4.276544
1.588208	239.587637	4.281549
2.105898	237.743298	4.286554
1.714409	234.434518	4.291558
1.820398	240.683595	4.296563
2.024578	242.895702	4.301568
1.691255	250.505933	4.306573
1.836278	255.762664	4.311578
1.940980	258.529380	4.316582
1.748735	268.053899	4.321587
2.001942	265.317192	4.326592
1.740168	269.318349	4.331597
1.783829	259.132575	4.336602
1.914246	264.473819	4.341606
2.040993	263.873099	4.346611
1.878585	264.933283	4.351616
1.838017	272.136883	4.356621
1.892380	268.101479	4.361626
2.079995	264.740409	4.366630
1.667089	268.641087	4.371635
2.022772	263.681984	4.376640
1.643740	268.978335	4.381645
2.481708	272.313518	4.386650
2.101245	274.664473	4.391654
2.013037	270.017650	4.396659
2.076795	276.989275	4.401664
2.058627	300.096839	4.406669
1.987842	298.765530	4.411674
2.123453	301.348941	4.416678
2.257850	298.423712	4.421683
2.330384	307.434158	4.426688
2.313351	298.469463	4.431693
2.394496	294.753446	4.436698
2.028424	309.487050	4.441702
2.473029	303.674135	4.446707
2.233612	306.391479	4.451712
2.103080	308.679149	4.456717
2.350616	305.589352	4.461722
2.064778	311.223714	4.466726
2.386566	305.542829	4.471731
2.474317	312.585090	4.476736
2.219582	306.560796	4.481741
2.488741	304.895740	4.486746
2.240674	312.091685	4.491750
2.479447	299.912644	4.496755
2.036128	307.398443	4.501760
2.128709	300.412838	4.506765
2.473618	307.626426	4.511770
2.379524	300.074592	4.516774
2.381843	302.046231	4.521779
2.460328	312.265958	4.526784
2.111895	313.373921	4.531789
2.175753	304.857200	4.536794
1.975312	307.629462	4.541798
2.455537	322.292992	4.546803
2.531318	329.898864	4.551808
2.377621	338.210921	4.556813
2.479667	326.789578	4.561818
2.394232	344.779963	4.566822
2.390347	344.329535	4.571827
2.494295	330.984827	4.576832
2.454787	335.943379	4.581837
2.960102	333.362052	4.586842
2.806283	344.092889	4.591846
2.610780	337.146881	4.596851
2.452901	337.735475	4.601856
2.276202	338.402568	4.606861
2.523281	334.087379	4.611866
2.618578	334.810074	4.616870
2.548122	331.063701	4.621875
2.530564	333.116188	4.626880
2.661220	340.333302	4.631885
2.812748	339.888713	4.636890
2.381285	346.981051	4.641894
2.861750	357.129508	4.646899
2.965825	358.609708	4.651904
2.905004	372.854934	4.656909
3.175801	354.012982	4.661914
2.666192	346.910002	4.666918
3.001218	336.828669	4.671923
2.929014	341.482225	4.676928
2.832893	335.404027	4.681933
2.845138	337.034607	4.686938
2.932007	346.692138	4.691942
2.871608	348.794346	4.696947
3.173595	336.692228	4.701952
2.796651	342.335373	4.706957
3.133245	335.310530	4.711962
2.864588	346.224963	4.716966
3.109233	336.651741	4.721971
2.632091	336.272182	4.726976
2.695815	341.698300	4.731981
3.250387	350.115084	4.736986
3.195875	356.079585	4.741990
3.120931	342.518608	4.746995
3.169093	347.239852	4.752000
2.788768	336.917624	4.757005
3.043793	338.138983	4.762010
2.553092	349.995766	4.767014
3.062398	353.509713	4.772019
3.255652	366.526470	4.777024
3.174540	375.410646	4.782029
3.033539	372.792084	4.787034
2.978487	377.338025	4.792038
3.011488	368.286858	4.797043
2.832853	384.027094	4.802048
3.184398	379.272490	4.807053
3.395164	370.548672	4.812058
2.883771	382.442848	4.817062
3.047085	374.366456	4.822067
3.087455	373.640320	4.827072
2.839664	374.985003	4.832077
2.888201	368.276223	4.837082
3.075357	376.473249	4.842086
3.147209	368.307614	4.847091
3.320656	389.927628	4.852096
3.609969	401.502548	4.857101
3.242132	376.732132	4.862106
3.331032	372.768140	4.867110
3.492529	374.473468	4.872115
3.524433	369.961832	4.877120
3.271286	374.307717	4.882125
3.375264	373.699317	4.887130
3.018249	378.861225	4.892134
3.163255	389.257063	4.897139
3.567217	399.979049	4.902144
3.465005	401.532486	4.907149
3.494500	408.976350	4.912154
3.586329	401.534579	4.917158
3.439356	408.601938	4.922163
3.604981	404.372642	4.927168
3.394841	403.625825	4.932173
3.645244	397.472264	4.937178
3.715510	406.725868	4.942182
3.300229	394.729257	4.947187
3.408888	386.069699	4.952192
3.359849	402.272956	4.957197
3.703255	399.945565	4.962202
3.802855	409.165700	4.967206
3.636076	402.788171	4.972211
3.728984	399.143986	4.977216
3.735526	408.136212	4.982221
3.457351	391.293769	4.987226
3.497444	393.542936	4.992230
3.766479	404.211687	4.997235
3.826350	394.068529	5.002240
3.686357	400.465755	5.007245
3.828533	385.754816	5.012250
3.659724	380.217501	5.017254
3.885524	381.945926	5.022259
3.437637	372.701864	5.027264
3.768580	391.494402	5.032269
3.832545	394.000891	5.037274
3.562331	398.963920	5.042278
3.916269	396.974601	5.047283
4.278617	403.970644	5.052288
3.749677	392.922907	5.057293
3.393519	376.016630	5.062298
3.932327	385.637039	5.067302
3.903680	396.824940	5.072307
4.146566	403.019642	5.077312
3.663351	384.677254	5.082317
3.915673	378.492795	5.087322
3.815393	384.467451	5.092326
3.790367	394.321933	5.097331
3.736361	394.405510	5.102336
3.823890	407.219186	5.107341
3.975827	404.239133	5.112346
3.835026	407.066657	5.117350
3.871066	407.469614	5.122355
3.780495	405.763867	5.127360
3.636135	408.553106	5.132365
3.818228	407.808039	5.137370
3.433290	413.420959	5.142374
3.474597	415.748863	5.147379
3.642226	415.192873	5.152384
3.562901	437.024915	5.157389
4.110547	433.894081	5.162394
4.187700	442.617897	5.167398
3.959955	441.066289	5.172403
4.115931	438.996474	5.177408
4.181850	440.777034	5.182413
4.388977	441.404451	5.187418
3.902232	447.899964	5.192422
4.158605	447.720205	5.197427
4.096885	440.640500	5.202432
4.175473	450.065818	5.207437
4.400537	443.965966	5.212442
4.007780	447.682195	5.217446
4.039242	440.006097	5.222451
4.341718	436.111904	5.227456
4.344250	443.510915	5.232461
4.419933	440.723060	5.237466
4.336949	447.011012	5.242470
4.284018	445.466568	5.247475
4.391197	435.855663	5.252480
4.125545	444.130666	5.257485
4.303746	442.574788	5.262490
4.268813	444.115312	5.267494
4.224190	436.692962	5.272499
4.182836	440.292982	5.277504
4.195928	436.485979	5.282509
4.127409	429.803068	5.287514
4.332270	440.892737	5.292518
4.550875	436.590327	5.297523
4.447593	443.278090	5.302528
4.494967	444.083517	5.307533
4.742320	439.357396	5.312538
4.174493	447.288354	5.317542
4.281394	443.529556	5.322547
4.419084	447.439154	5.327552
4.146993	444.700993	5.332557
4.256343	448.735661	5.337562
4.547226	462.406888	5.342566
4.423763	466.762109	5.347571
4.631056	464.582360	5.352576
4.623243	472.639446	5.357581
4.826173	473.236577	5.362586
4.645896	459.511191	5.367590
4.444431	462.232736	5.372595
4.630448	452.988247	5.377600
4.517154	469.095257	5.382605
4.577964	463.281505	5.387610
4.537363	466.379180	5.392614
4.641085	470.633437	5.397619
4.690578	465.352003	5.402624
4.707079	472.993810	5.407629
4.891913	464.265353	5.412634
4.442753	471.004680	5.417638
4.610050	473.829151	5.422643
4.364660	464.823041	5.427648
4.467064	476.825026	5.432653
4.413067	463.155688	5.437658
3.771529	475.414855	5.442662
4.084725	482.116749	5.447667
4.430988	489.201731	5.452672
4.544441	499.480716	5.457677
4.867779	496.889832	5.462682
4.904910	505.225239	5.467686
4.846616	501.901484	5.472691
5.119990	500.887125	5.477696
5.089389	503.530654	5.482701
5.080053	489.611959	5.487706
4.979631	497.079155	5.492710
5.001142	497.449196	5.497715
5.216592	501.443418	5.502720
5.078034	500.552328	5.507725
5.094624	491.763703	5.512730
5.073046	504.381216	5.517734
5.148493	490.768960	5.522739
5.091869	482.039824	5.527744
4.588256	477.664195	5.532749
5.151106	482.177114	5.537754
4.897398	488.648066	5.542758
5.161650	493.785281	5.547763
5.061487	499.901454	5.552768
5.286171	503.643329	5.557773
5.095451	484.013297	5.562778
4.787012	476.276641	5.567782
4.875009	487.741694	5.572787
4.888247	490.422955	5.577792
4.563996	498.019373	5.582797
4.879949	501.823885	5.587802
4.942068	495.305009	5.592806
4.917422	497.554255	5.597811
5.032547	500.188059	5.602816
4.840379	498.088661	5.607821
5.055425	496.623175	5.612826
4.670600	504.295142	5.617830
4.645938	514.237850	5.622835
5.052667	526.842673	5.627840
4.984784	531.975697	5.632845
5.408585	525.105251	5.637850
5.223950	527.248776	5.642854
5.243542	523.178806	5.647859
5.575846	524.578408	5.652864
5.120108	532.654245	5.657869
5.726787	527.636525	5.662874
5.461374	539.059889	5.667878
5.455095	530.414745	5.672883
5.448143	525.024234	5.677888
5.367074	538.955052	5.682893
5.683137	527.258751	5.687898
5.319765	527.986561	5.692902
5.558654	530.015554	5.697907
5.938701	531.609128	5.702912
5.717417	521.861733	5.707917
5.523691	507.743853	5.712922
5.354266	502.177785	5.717926
5.188470	503.893711	5.722931
5.348923	512.615417	5.727936
5.472204	525.897476	5.732941
5.619606	528.192831	5.737946
5.388940	533.939501	5.742950
5.458541	523.753205	5.747955
5.443882	526.845413	5.752960
5.437270	530.206644	5.757965
5.423731	530.645046	5.762970
5.241740	533.254250	5.767974
5.297824	529.489638	5.772979
5.279807	527.764562	5.777984
5.346272	535.429305	5.782989
5.298841	530.663168	5.787994
5.759706	527.067348	5.792998
5.470935	533.623061	5.798003
5.479707	544.668510	5.803008
5.703048	566.422791	5.808013
6.034996	558.776404	5.813018
5.691392	553.834336	5.818022
5.457338	546.182221	5.823027
5.400094	553.088954	5.828032
5.429766	579.117926	5.833037
5.900886	567.333559	5.838042
5.442477	568.592560	5.843046
5.836523	578.369476	5.848051
5.536832	573.992415	5.853056
5.419261	566.224700	5.858061
5.705789	563.812573	5.863066
5.365228	573.432091	5.868070
5.737404	574.808716	5.873075
5.696185	575.008383	5.878080
6.029838	596.092231	5.883085
6.219315	586.082200	5.888090
5.729699	573.595331	5.893094
5.560255	569.014954	5.898099
5.613834	582.464896	5.903104
6.035638	591.404845	5.908109
6.265141	588.805803	5.913114
5.916006	596.397706	5.918118
6.070475	594.376665	5.923123
6.309670	590.513437	5.928128
6.297761	573.463702	5.933133
5.944417	563.786693	5.938138
6.073280	576.599585	5.943142
5.877227	566.006922	5.948147
5.700087	562.225074	5.953152
5.876832	589.077282	5.958157
6.029335	584.284533	5.963162
6.091592	594.811235	5.968166
6.242765	592.353040	5.973171
6.349106	584.971137	5.978176
6.183431	594.171371	5.983181
6.149038	577.959313	5.988186
6.335151	579.436212	5.993190
5.835896	576.120140	5.998195
6.211805	578.233606	6.003200
6.265963	595.599675	6.008205
6.175773	580.531757	6.013210
5.896197	583.060037	6.018214
5.939861	585.651222	6.023219
6.378756	584.672796	6.028224
6.136564	590.946319	6.033229
6.447631	590.657056	6.038234
5.978166	594.285772	6.043238
6.343841	589.539619	6.048243
6.461127	597.845818	6.053248
6.116572	583.799416	6.058253
6.503313	573.974789	6.063258
5.963489	580.044406	6.068262
5.975487	565.114691	6.073267
6.231780	569.533749	6.078272
6.090661	580.508334	6.083277
5.867477	583.545293	6.088282
6.049669	590.642690	6.093286
6.115500	596.073680	6.098291
6.417116	594.766325	6.103296
6.197049	596.274174	6.108301
6.460876	594.390923	6.113306
6.259573	592.709807	6.118310
6.062187	578.704360	6.123315
6.216958	567.279833	6.128320
5.897473	574.040751	6.133325
6.059136	581.888475	6.138330
6.169566	598.027246	6.143334
6.502707	598.161371	6.148339
6.280384	586.471886	6.153344
6.028706	581.877692	6.158349
6.390451	564.233671	6.163354
6.175747	565.603281	6.168358
6.336457	568.824526	6.173363
6.268280	570.249204	6.178368
5.988710	581.395116	6.183373
6.525185	569.961254	6.188378
6.387903	573.205402	6.193382
6.082140	573.233183	6.198387
6.225456	570.537511	6.203392
5.890670	571.724930	6.208397
6.000532	567.956139	6.213402
6.211693	570.143062	6.218406
6.357039	567.886925	6.223411
6.275429	569.535242	6.228416
6.232709	566.896820	6.233421
6.268456	572.218720	6.238426
6.198693	579.560698	6.243430
6.268553	569.941090	6.248435
6.301147	567.578312	6.253440
5.844680	575.158772	6.258445
6.184046	561.705616	6.263450
6.099169	576.292858	6.268454
6.238428	570.798395	6.273459
6.419599	570.816192	6.278464
6.325923	570.296756	6.283469
6.340732	570.278163	6.288474
6.313897	572.968639	6.293478
6.038024	571.483399	6.298483
6.303172	569.194399	6.303488
6.176395	574.415534	6.308493
6.375517	567.365200	6.313498
6.144138	575.149141	6.318502
6.220105	575.766511	6.323507
6.199505	563.897213	6.328512
6.183987	564.776407	6.333517
6.418393	569.127257	6.338522
6.423579	573.464362	6.343526
6.359787	562.174306	6.348531
6.553201	570.482882	6.353536
6.241321	551.341905	6.358541
6.370957	537.741552	6.363546
6.048785	536.431129	6.368550
6.240113	536.076640	6.373555
5.895400	527.702639	6.378560
5.618899	542.826374	6.383565
6.045182	546.576515	6.388570
6.124477	568.671382	6.393574
6.023139	570.814539	6.398579
6.299259	565.002195	6.403584
6.136543	570.039636	6.408589
6.513453	565.523898	6.413594
6.597520	569.204613	6.418598
6.223584	552.706422	6.423603
6.351118	536.219933	6.428608
5.858183	539.944287	6.433613
6.127070	533.268214	6.438618
6.076874	544.513267	6.443622
5.899796	556.613100	6.448627
6.286142	562.722541	6.453632
6.208770	568.813654	6.458637
6.235834	571.314245	6.463642
5.966987	571.325651	6.468646
6.056710	576.662098	6.473651
6.520592	569.136733	6.478656
6.111466	581.671860	6.483661
6.333633	571.976708	6.488666
6.135131	561.578241	6.493670
6.070638	557.421937	6.498675
6.415685	559.326200	6.503680
5.865865	559.455372	6.508685
6.230725	561.374707	6.513690
5.897920	571.701784	6.518694
6.141469	567.631423	6.523699
6.235120	569.891283	6.528704
6.057372	568.627984	6.533709
6.386541	570.625457	6.538714
6.420863	573.633785	6.543718
6.215641	563.192225	6.548723
6.220982	562.182976	6.553728
5.851838	551.524261	6.558733
6.149950	562.555556	6.563738
6.027113	566.280004	6.568742
5.927287	574.440787	6.573747
6.588991	569.129576	6.578752
6.361772	577.639435	6.583757
6.395343	561.974020	6.588762
6.197573	549.508701	6.593766
5.839967	539.262301	6.598771
6.361098	545.962944	6.603776
5.778249	555.876549	6.608781
5.999827	558.255137	6.613786
6.056164	566.567663	6.618790
6.346270	574.073042	6.623795
6.182745	569.472148	6.628800
6.615980	581.222882	6.633805
6.343892	564.415948	6.638810
6.079869	554.561152	6.643814
5.912264	546.556242	6.648819
6.046862	552.276771	6.653824
5.944597	573.399619	6.658829
6.359584	573.816595	6.663834
6.204825	575.103856	6.668838
6.321879	574.177145	6.673843
6.196824	575.830091	6.678848
6.190798	579.901067	6.683853
6.285092	565.851082	6.688858
6.030686	569.862936	6.693862
6.054642	569.404734	6.698867
6.127823	571.687323	6.703872
6.211451	568.045622	6.708877
6.285179	569.818984	6.713882
6.071197	577.124851	6.718886
5.862496	567.482499	6.723891
6.024683	563.673668	6.728896
5.807315	575.151659	6.733901
6.050449	575.863501	6.738906
6.098460	571.867946	6.743910
6.154998	570.929944	6.748915
6.509790	572.128881	6.753920
5.958874	576.153920	6.758925
6.233589	565.761946	6.763930
6.064769	570.460973	6.768934
6.175858	572.180195	6.773939
5.841643	562.597704	6.778944
5.931912	567.426697	6.783949
6.261749	567.773114	6.788954
5.969511	565.202059	6.793958
5.988796	567.668811	6.798963
5.975295	564.852287	6.803968
5.779961	577.773329	6.808973
6.257855	570.424038	6.813978
6.119851	584.028847	6.818982
6.279204	583.235045	6.823987
6.235137	577.206743	6.828992
6.387460	574.283427	6.833997
6.284409	569.437093	6.839002
6.239606	567.398731	6.844006
5.954350	575.658303	6.849011
6.254820	576.086941	6.854016
6.170247	579.349003	6.859021
6.060298	568.339309	6.864026
6.132030	571.219881	6.869030
5.993363	576.243671	6.874035
6.201802	577.122683	6.879040
6.251900	569.966385	6.884045
6.205287	577.059828	6.889050
6.453866	571.120219	6.894054
6.066406	581.183235	6.899059
6.026035	580.738447	6.904064
6.109748	578.565332	6.909069
6.464729	567.974369	6.914074
6.240917	574.517171	6.919078
6.238475	578.270823	6.924083
6.788406	575.205889	6.929088
5.845820	574.210929	6.934093
6.327866	578.145632	6.939098
6.006364	575.180400	6.944102
5.979790	576.197787	6.949107
6.224892	570.731975	6.954112
6.170611	577.942132	6.959117
6.294640	575.394106	6.964122
6.037128	582.832889	6.969126
5.989203	577.537159	6.974131
5.992295	568.752501	6.979136
5.902231	572.984409	6.984141
6.162044	570.153805	6.989146
6.252942	583.294653	6.994150
6.174326	577.850079	6.999155
6.197081	576.976083	7.004160
6.229308	577.405724	7.009165
6.361367	564.928008	7.014170
6.012147	572.647789	7.019174
6.135940	573.011551	7.024179
6.251038	564.185655	7.029184
5.774269	576.006952	7.034189
6.249108	568.173897	7.039194
6.180842	574.207263	7.044198
6.250761	574.722228	7.049203
6.407022	570.305977	7.054208
6.063177	580.427287	7.059213
6.339536	561.472073	7.064218
6.220114	566.411962	7.069222
6.317737	575.755269	7.074227
6.498617	575.575379	7.079232
6.611648	586.175563	7.084237
6.641183	578.543920	7.089242
6.322290	577.376811	7.094246
6.671918	576.813964	7.099251
6.696536	567.045556	7.104256
6.032941	555.516586	7.109261
6.089941	533.749330	7.114266
6.055335	542.142419	7.119270
6.058431	536.546191	7.124275
6.374553	534.029117	7.129280
6.109506	533.712903	7.134285
6.122638	536.555613	7.139290
5.960453	549.415098	7.144294
6.458629	561.180716	7.149299
6.190633	541.689705	7.154304
6.140218	536.970829	7.159309
6.072903	530.380030	7.164314
6.157143	544.663752	7.169318
6.257417	543.279034	7.174323
6.512448	544.498830	7.179328
5.959651	537.314702	7.184333
5.973282	536.206004	7.189338
6.068050	542.526131	7.194342
6.285150	564.790381	7.199347
6.303700	553.032223	7.204352
6.321465	550.133562	7.209357
5.932406	538.974149	7.214362
6.006620	546.081512	7.219366
5.958254	564.459508	7.224371
6.355428	561.511832	7.229376
6.216296	567.240792	7.234381
6.355704	558.324438	7.239386
5.942364	555.838166	7.244390
6.223905	563.859225	7.249395
6.455689	567.389970	7.254400
6.099241	547.399924	7.259405
6.312444	540.741356	7.264410
6.437195	532.624695	7.269414
6.235243	535.442833	7.274419
6.156457	535.368301	7.279424
5.799187	548.575635	7.284429
5.988433	529.329798	7.289434
6.186552	534.342998	7.294438
6.039161	538.844680	7.299443
5.959859	549.457743	7.304448
6.003441	567.191399	7.309453
6.382917	567.095646	7.314458
6.472397	564.492365	7.319462
6.164975	549.140956	7.324467
6.258339	531.387883	7.329472
5.956345	546.153922	7.334477
6.073807	552.596987	7.339482
6.494049	562.944997	7.344486
6.154601	556.177637	7.349491
6.433863	537.937328	7.354496
6.305080	544.280461	7.359501
6.360901	536.120747	7.364506
6.135986	534.430720	7.369510
6.074956	534.612750	7.374515
6.226448	535.186630	7.379520
6.180885	539.411949	7.384525
6.082871	532.364656	7.389530
6.140612	534.717287	7.394534
5.954931	532.373096	7.399539
6.008163	533.886992	7.404544
5.854049	548.896533	7.409549
6.311122	557.756817	7.414554
6.455740	570.023423	7.419558
5.731982	557.311496	7.424563
6.420641	559.406521	7.429568
6.393309	555.500211	7.434573
6.168068	547.593449	7.439578
5.851812	531.568422	7.444582
6.091843	555.834028	7.449587
6.561246	551.445852	7.454592
6.201755	551.082917	7.459597
6.316846	541.946816	7.464602
6.451010	535.545053	7.469606
6.094722	543.429388	7.474611
6.087236	538.849236	7.479616
6.155943	546.632018	7.484621
5.918301	537.386590	7.489626
6.286891	542.920168	7.494630
6.089369	534.551785	7.499635
6.260797	530.479956	7.504640
5.855749	539.075483	7.509645
6.118111	530.463803	7.514650
5.941639	549.313323	7.519654
6.042495	559.508196	7.524659
6.442795	570.675711	7.529664
5.946574	574.267017	7.534669
6.370256	571.413817	7.539674
5.957963	582.997897	7.544678
6.325618	574.291203	7.549683
6.471290	568.985125	7.554688
5.947743	562.535771	7.559693
6.353553	554.171864	7.564698
6.078633	551.242338	7.569702
5.707159	551.784216	7.574707
6.143043	557.282185	7.579712
6.378209	573.582421	7.584717
6.322086	574.955373	7.589722
6.053250	573.352735	7.594726
6.158543	568.517092	7.599731
6.322907	565.563367	7.604736
6.242143	575.196109	7.609741
6.316788	558.645733	7.614746
5.915913	559.000666	7.619750
6.241924	561.948258	7.624755
6.174014	572.555109	7.629760
6.147872	570.998126	7.634765
5.847241	570.280691	7.639770
6.110128	568.543039	7.644774
5.842178	571.987811	7.649779
6.168157	571.468940	7.654784
6.016923	576.044285	7.659789
6.240917	569.650722	7.664794
6.314063	562.400822	7.669798
6.064416	575.815522	7.674803
6.120361	558.841200	7.679808
5.990595	570.189435	7.684813
5.874787	569.015536	7.689818
6.100235	562.656073	7.694822
5.887719	582.757407	7.699827
6.260277	565.344849	7.704832
6.158183	573.746368	7.709837
6.271796	571.642700	7.714842
6.051347	562.546560	7.719846
5.988626	576.153498	7.724851
6.355112	566.662774	7.729856
6.328968	574.056531	7.734861
6.149297	572.830059	7.739866
6.070608	571.651592	7.744870
6.039263	576.062237	7.749875
6.351482	573.067056	7.754880
6.042353	572.764258	7.759885
6.175867	571.500726	7.764890
6.328261	572.943345	7.769894
6.379437	568.626787	7.774899
6.256685	562.957455	7.779904
6.161928	572.383924	7.784909
6.443697	564.082980	7.789914
6.613869	572.459739	7.794918
6.096806	573.759632	7.799923
6.592620	565.779244	7.804928
6.206535	577.592828	7.809933
6.082388	577.550869	7.814938
6.276105	583.482247	7.819942
6.221138	570.004789	7.824947
6.294006	567.649354	7.829952
6.315613	566.917042	7.834957
6.221051	548.569501	7.839962
6.022260	552.348753	7.844966
5.784451	555.178554	7.849971
6.088677	561.417826	7.854976
5.880410	578.597232	7.859981
6.247614	575.687275	7.864986
6.429029	577.252965	7.869990
5.928341	578.345506	7.874995
6.097062	574.541312	7.880000
5.975369	573.336419	7.885005
6.268228	566.126505	7.890010
6.379061	573.666503	7.895014
6.304194	571.807962	7.900019
6.029689	569.208908	7.905024
5.743155	577.486848	7.910029
6.313411	576.854906	7.915034
6.185518	573.860771	7.920038
6.066105	572.397775	7.925043
6.282903	568.599830	7.930048
5.896697	577.083128	7.935053
6.165017	574.781762	7.940058
6.233344	580.583726	7.945062
6.179602	581.545620	7.950067
6.200406	579.792206	7.955072
5.891423	582.464677	7.960077
6.061094	581.693637	7.965082
5.847438	578.281135	7.970086
5.961911	575.193980	7.975091
6.240849	571.500991	7.980096
6.159908	577.888117	7.985101
6.136477	577.656414	7.990106
6.514335	569.147741	7.995110
5.876037	583.835314	8.000115
6.384098	571.445769	8.005133
5.670814	580.117056	8.010150
5.920018	582.484323	8.015168
5.995448	578.203671	8.020186
6.027785	592.366061	8.025203
6.509941	594.262698	8.030221
6.280827	588.973491	8.035238
6.373235	588.289380	8.040256
6.369886	578.120219	8.045274
6.198792	582.127444	8.050291
6.379058	576.763563	8.055309
6.367857	573.072808	8.060326
6.286317	570.467443	8.065344
6.364839	572.337615	8.070362
6.132302	574.784455	8.075379
6.145177	572.542562	8.080397
6.203747	570.223030	8.085414
6.416463	572.103459	8.090432
6.390209	575.923324	8.095450
6.323524	582.997687	8.100467
6.305194	570.669157	8.105485
6.487758	578.395699	8.110502
6.423362	574.353738	8.115520
6.308217	574.220691	8.120538
6.282399	577.699170	8.125555
6.427338	573.593020	8.130573
5.885617	579.513650	8.135590
6.246638	577.230051	8.140608
6.465380	571.253741	8.145626
5.876453	574.121972	8.150643
6.143054	568.933351	8.155661
6.290865	581.828471	8.160678
6.274176	577.848879	8.165696
6.121073	568.301135	8.170714
5.939073	580.227712	8.175731
6.056621	589.895992	8.180749
6.397486	603.174093	8.185766
6.539761	611.708646	8.190784
6.251101	607.085548	8.195802
6.294645	609.366803	8.200819
6.530563	608.599285	8.205837
6.226636	607.348168	8.210854
6.009146	606.437832	8.215872
6.625247	605.851830	8.220890
6.315096	607.020081	8.225907
6.459963	604.298092	8.230925
6.311136	605.799249	8.235942
6.409483	602.809195	8.240960
6.316245	605.180024	8.245978
6.376941	613.981219	8.250995
6.630878	605.672259	8.256013
6.207577	605.860890	8.261030
6.317168	608.461698	8.266048
6.554474	601.767785	8.271066
6.114273	613.539322	8.276083
6.587852	613.134390	8.281101
6.253355	609.120021	8.286118
6.243369	621.117351	8.291136
6.541941	606.371321	8.296154
6.537761	608.934869	8.301171
6.418126	606.681452	8.306189
6.362946	613.535238	8.311206
6.469013	606.496938	8.316224
6.602988	600.837389	8.321242
6.399305	609.602247	8.326259
6.540315	606.670280	8.331277
6.632357	604.627858	8.336294
6.363808	608.095753	8.341312
6.645432	608.193048	8.346330
6.393884	614.266218	8.351347
6.768609	613.530829	8.356365
6.648456	615.885842	8.361382
6.387558	606.805696	8.366400
6.556302	607.426175	8.371418
6.111151	612.355697	8.376435
6.561129	600.221625	8.381453
6.278289	610.046369	8.386470
6.374192	609.803577	8.391488
6.731517	630.013342	8.396506
6.349253	636.862643	8.401523
6.594789	629.172540	8.406541
6.573988	636.840864	8.411558
6.465450	638.490265	8.416576
6.870321	640.521548	8.421594
6.949343	642.591829	8.426611
6.691646	623.242540	8.431629
6.642372	609.673715	8.436646
6.302043	610.035208	8.441664
6.879251	615.793205	8.446682
6.641421	624.026951	8.451699
6.950213	623.437116	8.456717
6.942124	613.756677	8.461734
6.585082	612.986566	8.466752
6.919052	600.381974	8.471770
5.986442	616.921341	8.476787
6.194964	614.637204	8.481805
6.416050	623.912992	8.486822
6.521978	642.264532	8.491840
6.809902	633.135220	8.496858
6.471436	643.738830	8.501875
6.705342	638.372344	8.506893
6.964879	645.482277	8.511910
6.406819	638.228958	8.516928
7.099048	641.496627	8.521946
6.953512	640.878487	8.526963
6.958690	638.824855	8.531981
6.876915	642.311433	8.536998
6.733086	630.820511	8.542016
6.691957	617.022591	8.547034
6.663498	635.974880	8.552051
6.567159	645.911471	8.557069
6.380513	640.336100	8.562087
6.397001	646.961315	8.567104
6.855971	637.139549	8.572122
6.390010	643.958620	8.577139
6.618534	637.822802	8.582157
6.885695	645.811139	8.587175
6.633862	643.072947	8.592192
6.884605	633.867711	8.597210
6.787704	642.742850	8.602227
6.592020	642.255841	8.607245
6.616038	648.308195	8.612263
6.511506	647.392733	8.617280
6.736146	642.679509	8.622298
6.662838	651.183250	8.627315
6.862929	647.015393	8.632333
7.087061	661.238403	8.637351
6.936426	656.874699	8.642368
6.950447	646.521528	8.647386
6.834468	650.520037	8.652403
6.606316	638.672428	8.657421
6.725496	649.374461	8.662439
6.991906	661.368570	8.667456
7.331305	659.661337	8.672474
7.121539	651.189587	8.677491
7.008308	645.925263	8.682509
7.018109	644.834384	8.687527
7.015752	640.811264	8.692544
6.926711	639.371225	8.697562
7.201354	639.847800	8.702579
7.188736	647.547055	8.707597
6.995758	644.234786	8.712615
6.562560	652.405235	8.717632
6.948302	643.901606	8.722650
6.979107	645.087018	8.727667
6.970264	642.925085	8.732685
7.210543	638.420282	8.737703
6.960737	643.764680	8.742720
7.276244	646.067635	8.747738
7.172993	646.396957	8.752755
7.059104	652.329244	8.757773
6.713907	645.721927	8.762791
7.227532	639.460557	8.767808
7.296638	642.213931	8.772826
7.130881	651.836845	8.777843
6.969026	652.679579	8.782861
6.937791	640.781448	8.787879
6.700731	650.398454	8.792896
7.220509	637.681966	8.797914
7.183695	646.029869	8.802931
6.942164	643.617706	8.807949
6.954981	642.736549	8.812967
6.770676	649.867818	8.817984
7.203512	641.719164	8.823002
7.121641	648.537033	8.828019
6.827200	645.659844	8.833037
7.346942	637.780443	8.838055
7.070948	646.471475	8.843072
6.846974	641.360325	8.848090
6.965237	651.221031	8.853107
7.211977	642.982530	8.858125
7.107968	647.329427	8.863143
6.904572	638.767659	8.868160
7.088353	639.551976	8.873178
6.595175	648.726188	8.878195
6.914917	644.929436	8.883213
7.297756	642.100125	8.888231
6.853194	656.014596	8.893248
7.176000	634.190978	8.898266
7.369269	643.865847	8.903283
7.332913	646.100106	8.908301
7.194756	648.962599	8.913319
6.861595	641.648220	8.918336
7.173302	637.596125	8.923354
6.972371	640.278473	8.928371
7.163363	643.203974	8.933389
7.179208	632.318065	8.938407
7.145618	654.584783	8.943424
7.311964	643.221810	8.948442
7.346758	645.376378	8.953459
7.031884	650.510309	8.958477
7.378966	642.898653	8.963495
6.964819	644.193175	8.968512
7.140024	655.103243	8.973530
7.127442	663.065869	8.978547
7.345051	671.238987	8.983565
7.337101	668.360217	8.988583
7.330644	677.879608	8.993600
7.692905	666.073967	8.998618
7.263993	647.349613	9.003635
6.847165	643.146126	9.008653
7.470458	650.153114	9.013671
7.301208	660.606675	9.018688
7.332790	653.604112	9.023706
7.161026	646.513775	9.028723
7.401598	663.237442	9.033741
7.611251	653.187282	9.038759
7.154521	650.478885	9.043776
7.184706	637.305907	9.048794
7.097338	647.354391	9.053811
7.043754	668.361335	9.058829
7.507485	666.626820	9.063847
7.538732	678.937032	9.068864
7.429146	676.753786	9.073882
7.650852	678.081987	9.078899
7.009678	666.086622	9.083917
7.792563	667.449841	9.088935
7.142074	660.962357	9.093952
7.399845	663.738033	9.098970
7.738157	671.964192	9.103987
7.799661	652.133691	9.109005
7.530449	644.174708	9.114023
7.254531	637.133706	9.119040
7.260077	630.059485	9.124058
7.649487	631.618163	9.129075
7.490823	637.824377	9.134093
7.459310	634.314124	9.139111
7.315948	636.458234	9.144128
7.317017	636.167172	9.149146
7.039241	640.547959	9.154163
7.330066	656.025584	9.159181
7.767627	663.348157	9.164199
7.663753	668.765047	9.169216
7.482282	654.390371	9.174234
7.312215	643.772822	9.179251
7.174390	662.704674	9.184269
7.145777	670.735899	9.189287
7.444789	670.941921	9.194304
7.073394	673.432438	9.199322
7.490406	673.006756	9.204339
7.398343	683.793789	9.209357
7.588946	670.098975	9.214375
7.063375	669.392003	9.219392
7.255171	676.517301	9.224410
7.312950	667.430016	9.229427
7.120676	674.523642	9.234445
7.633103	687.289580	9.239463
7.616627	698.284565	9.244480
7.823061	709.047777	9.249498
7.731277	692.958517	9.254515
7.385076	690.102685	9.259533
7.923436	678.555256	9.264551
7.672497	681.791133	9.269568
7.695371	674.916175	9.274586
7.818998	676.013389	9.279603
7.563112	682.601050	9.284621
7.559656	676.101294	9.289639
7.865400	679.811882	9.294656
7.234685	671.727915	9.299674
7.604342	679.949281	9.304691
7.541384	681.057708	9.309709
7.517530	694.626582	9.314727
7.973776	691.806759	9.319744
7.847422	692.401308	9.324762
7.806603	684.824733	9.329779
7.614058	681.492699	9.334797
7.720676	680.632620	9.339815
7.562357	673.886085	9.344832
7.506110	687.774076	9.349850
7.893954	685.969060	9.354867
7.608234	687.404513	9.359885
7.800313	683.585195	9.364903
7.441085	694.410176	9.369920
7.572361	702.084057	9.374938
7.945830	701.980131	9.379955
7.859108	705.312041	9.384973
7.807802	708.843979	9.389991
7.831156	712.397412	9.395008
7.767115	700.485574	9.400026
7.617960	704.394322	9.405043
7.378518	705.190264	9.410061
8.093239	706.892706	9.415079
7.919807	703.921653	9.420096
8.006147	713.070605	9.425114
8.157407	706.719615	9.430131
7.741770	691.146947	9.435149
7.517850	677.029461	9.440167
7.630065	692.230025	9.445184
8.015887	709.105270	9.450202
7.954862	711.109386	9.455219
7.776109	715.245070	9.460237
8.378138	699.976290	9.465255
7.788573	698.382331	9.470272
7.524090	683.576324	9.475290
7.986660	699.536939	9.480307
7.853552	706.541653	9.485325
7.754695	708.499675	9.490343
7.748902	715.738807	9.495360
7.915185	715.627067	9.500378
8.152495	711.160921	9.505395
7.715237	717.511718	9.510413
7.665833	701.269772	9.515431
7.862466	707.124285	9.520448
7.823916	711.089124	9.525466
7.879196	709.294295	9.530483
7.765820	706.479035	9.535501
7.823059	718.607426	9.540519
7.891357	709.517193	9.545536
7.935891	707.113552	9.550554
7.793346	710.249208	9.555571
7.881191	709.149337	9.560589
7.813251	701.871320	9.565607
7.773710	709.251069	9.570624
7.799310	711.949852	9.575642
7.888019	718.465901	9.580659
7.974099	732.470513	9.585677
7.920729	738.492413	9.590695
8.330578	743.823867	9.595712
8.297470	742.092093	9.600730
8.020944	717.804764	9.605747
8.010413	729.672749	9.610765
7.727466	726.906823	9.615783
7.812348	736.032408	9.620800
7.606851	750.412858	9.625818
7.760975	742.909479	9.630835
7.773977	741.111019	9.635853
8.149862	744.678126	9.640871
8.240776	742.116415	9.645888
8.032853	750.928312	9.650906
8.534451	742.817428	9.655923
8.304954	738.104577	9.660941
8.138124	743.614983	9.665959
8.562504	736.173543	9.670976
7.962801	742.926423	9.675994
8.196158	745.725447	9.681011
8.018046	751.438106	9.686029
7.871210	745.459671	9.691047
8.076277	736.940440	9.696064
8.310834	737.921658	9.701082
8.327885	737.000820	9.706099
8.138018	733.752973	9.711117
8.011839	742.050572	9.716135
8.023831	739.870412	9.721152
7.938532	742.320651	9.726170
8.204426	737.890313	9.731187
8.249297	745.491914	9.736205
8.246161	738.825553	9.741223
8.415712	736.631901	9.746240
7.937066	749.278160	9.751258
8.173415	738.938503	9.756275
8.499700	743.717293	9.761293
8.461421	746.315643	9.766311
8.441885	747.925122	9.771328
8.168203	741.635823	9.776346
8.351339	740.213496	9.781363
8.236948	752.003033	9.786381
8.238618	748.890778	9.791399
8.241346	747.042840	9.796416
8.307269	741.551979	9.801434
8.457497	735.490895	9.806451
8.059137	746.006269	9.811469
8.018320	746.394148	9.816487
8.326368	766.694728	9.821504
8.290868	774.962763	9.826522
8.582387	781.424390	9.831539
8.446692	789.797996	9.836557
8.606037	775.022108	9.841575
8.199167	764.648794	9.846592
7.970816	777.960282	9.851610
8.293709	779.592190	9.856627
8.459194	781.328900	9.861645
8.803629	784.424086	9.866663
8.748316	784.785628	9.871680
8.457671	772.645920	9.876698
8.435399	760.871206	9.881715
8.460996	765.169117	9.886733
8.369874	773.254641	9.891751
8.680940	773.047669	9.896768
8.366729	774.622880	9.901786
8.367517	763.922235	9.906803
8.277557	772.797284	9.911821
8.605593	775.243253	9.916839
8.809450	774.296205	9.921856
8.187976	775.153048	9.926874
8.627306	779.480479	9.931891
8.330969	781.063754	9.936909
8.420087	788.553724	9.941927
8.829133	774.706511	9.946944
8.650180	777.868680	9.951962
9.014340	774.662539	9.956979
8.534032	757.636426	9.961997
8.544830	756.309560	9.967015
8.517106	743.553143	9.972032
8.305461	764.059847	9.977050
8.951358	765.190656	9.982067
8.659054	765.444599	9.987085
8.459044	753.024560	9.992103
8.694939	762.813697	9.997120
8.613342	762.205239	10.002138
8.462610	755.753851	10.007155
8.611122	766.314895	10.012173
8.560910	773.607470	10.017191
8.600876	774.618550	10.022208
8.594590	776.549047	10.027226
8.821278	777.342605	10.032243
8.747325	772.481159	10.037261
8.472271	777.832737	10.042279
8.868082	778.938821	10.047296
8.360069	776.799491	10.052314
8.836430	776.969062	10.057331
8.987075	779.837297	10.062349
8.587468	772.481499	10.067367
8.627814	768.773500	10.072384
8.478740	771.283120	10.077402
8.676640	783.823284	10.082419
8.632618	774.407538	10.087437
8.338463	779.378049	10.092455
8.645583	770.809225	10.097472
8.484542	771.690607	10.102490
8.803633	775.260434	10.107507
8.650149	774.891425	10.112525
8.542970	775.115500	10.117543
8.688216	770.548054	10.122560
8.438054	780.253918	10.127578
8.584848	795.967726	10.132595
9.131482	802.805204	10.137613
9.124073	809.943079	10.142631
9.008230	784.731843	10.147648
8.868641	782.112631	10.152666
8.533558	776.748787	10.157683
8.918037	785.781881	10.162701
8.878736	799.490011	10.167719
9.242452	799.189286	10.172736
8.676162	788.459699	10.177754
8.717730	792.460896	10.182771
8.807676	797.739836	10.187789
8.920212	814.049459	10.192807
9.100265	802.957312	10.197824
9.026050	815.384302	10.202842
8.931992	800.509020	10.207859
8.943770	793.235082	10.212877
8.829449	810.018461	10.217895
9.081792	803.811708	10.222912
9.122319	807.159180	10.227930
9.343563	791.343557	10.232947
9.108575	787.936250	10.237965
8.623226	787.469840	10.242983
8.994185	774.920199	10.248000
8.716931	789.977883	10.253018
8.971067	796.352405	10.258035
9.157905	807.168927	10.263053
9.144205	804.715075	10.268071
9.066091	796.916681	10.273088
8.906175	799.280078	10.278106
9.087094	797.073906	10.283123
9.090617	806.770454	10.288141
8.987613	804.812465	10.293159
9.058294	807.410498	10.298176
8.861139	819.347247	10.303194
8.814016	806.980977	10.308211
8.935128	806.788925	10.313229
8.978645	805.288537	10.318247
9.119610	807.844225	10.323264
9.197574	809.288754	10.328282
9.011614	802.669568	10.333299
9.270399	812.517541	10.338317
9.241526	799.908504	10.343335
9.350084	807.584230	10.348352
9.489137	800.290001	10.353370
9.147114	811.494870	10.358387
9.186543	798.658394	10.363405
9.155442	807.272549	10.368423
9.403893	802.819886	10.373440
9.299162	802.840418	10.378458
9.106468	810.249119	10.383475
9.386309	802.855595	10.388493
9.309037	808.441347	10.393511
9.426801	805.037038	10.398528
9.144684	808.339123	10.403546
9.011822	808.913890	10.408563
9.183467	807.054902	10.413581
9.114919	808.346537	10.418599
9.490819	801.377240	10.423616
9.195284	804.294561	10.428634
9.254626	810.367899	10.433651
9.481748	804.449952	10.438669
9.118532	814.619021	10.443687
9.454941	807.250378	10.448704
9.329471	810.965477	10.453722
9.365394	814.278676	10.458739
9.189017	811.623820	10.463757
9.019037	815.532107	10.468775
9.501421	794.148350	10.473792
8.994987	808.418064	10.478810
9.004223	813.919812	10.483827
9.497946	801.810031	10.488845
9.100133	811.174636	10.493863
9.406542	801.453616	10.498880
9.106619	805.919214	10.503898
9.011051	817.553723	10.508915
9.326750	815.109888	10.513933
9.290807	837.433948	10.518951
9.352452	834.282219	10.523968
9.377283	837.189801	10.528986
9.626211	841.896004	10.534003
9.843547	838.056324	10.539021
9.547867	838.960792	10.544039
9.451796	818.530221	10.549056
9.655317	817.137188	10.554074
9.346248	822.713299	10.559091
9.519764	819.612729	10.564109
9.273234	830.506540	10.569127
9.532368	842.057137	10.574144
10.084255	829.786530	10.579162
9.670487	815.516900	10.584179
9.474229	804.420927	10.589197
9.582745	806.425326	10.594215
9.379152	804.848540	10.599232
9.520478	811.957851	10.604250
9.559326	825.181042	10.609267
9.795308	822.411842	10.614285
9.605214	823.330713	10.619303
9.619817	808.908269	10.624320
9.583659	808.292285	10.629338
9.449353	805.954068	10.634355
9.863622	824.672656	10.639373
9.673989	813.100409	10.644391
9.811567	805.172992	10.649408
9.750678	800.914852	10.654426
9.376523	803.435766	10.659443
9.374648	806.331624	10.664461
9.894527	822.158866	10.669479
9.695762	828.884760	10.674496
9.599900	832.996515	10.679514
9.615628	837.585434	10.684531
9.476697	832.057207	10.689549
9.593854	832.440975	10.694567
9.974729	835.784455	10.699584
9.903856	829.761521	10.704602
9.972145	841.721652	10.709619
10.270503	827.309288	10.714637
10.254454	826.820281	10.719655
9.904003	801.073883	10.724672
9.965020	809.073212	10.729690
9.768412	806.155975	10.734707
9.918094	803.473899	10.739725
9.762193	804.534343	10.744743
9.884218	802.642629	10.749760
9.626307	800.501642	10.754778
9.615858	800.771902	10.759795
9.466599	794.636772	10.764813
9.670160	805.613900	10.769831
9.668052	822.248404	10.774848
10.003020	824.394038	10.779866
9.861349	832.576934	10.784883
10.329000	826.508525	10.789901
9.807060	818.691886	10.794919
10.148337	801.398976	10.799936
9.931507	803.624168	10.804954
9.319390	808.463492	10.809971
10.134230	812.738594	10.814989
10.045406	825.309342	10.820007
9.919003	820.558923	10.825024
9.910730	823.268059	10.830042
9.922673	828.812274	10.835059
10.180909	823.240723	10.840077
9.903537	829.549736	10.845095
9.639450	825.612623	10.850112
10.041221	825.022935	10.855130
9.435282	838.667457	10.860147
9.869455	832.008559	10.865165
9.811401	839.390648	10.870183
9.946933	826.276833	10.875200
9.859426	833.345703	10.880218
10.061416	832.361167	10.885235
9.996817	832.449853	10.890253
9.960218	840.470087	10.895271
9.974893	831.674867	10.900288
9.983735	838.730541	10.905306
9.688292	833.539631	10.910323
10.258286	834.309807	10.915341
10.054798	846.597213	10.920359
10.118193	857.048798	10.925376
10.531034	868.690099	10.930394
10.032115	853.720791	10.935411
10.093838	834.196305	10.940429
10.257590	843.023869	10.945447
9.980981	842.760282	10.950464
10.520016	846.457475	10.955482
10.114867	850.042133	10.960499
10.153035	838.798268	10.965517
9.807429	831.207921	10.970535
10.165952	853.439127	10.975552
10.311150	855.958297	10.980570
10.150677	861.714136	10.985587
10.488987	858.796889	10.990605
10.404011	857.249666	10.995623
10.352710	857.905018	11.000640
10.563725	855.996988	11.005658
10.342049	846.759033	11.010675
10.266652	834.205307	11.015693
10.367973	830.855680	11.020711
10.595331	840.518335	11.025728
10.562719	837.397567	11.030746
10.305528	839.582206	11.035763
10.294307	826.042322	11.040781
10.084028	838.102118	11.045799
10.465404	832.082638	11.050816
10.479190	829.415186	11.055834
10.350941	835.747144	11.060851
10.282417	831.264682	11.065869
10.247243	830.752071	11.070887
10.400632	844.443293	11.075904
10.442570	830.356837	11.080922
10.241077	841.851826	11.085939
10.714947	856.639535	11.090957
10.611911	847.398075	11.095975
10.469581	841.600736	11.100992
10.714910	833.914110	11.106010
10.592457	831.144029	11.111027
10.454511	828.264708	11.116045
10.553917	827.180237	11.121063
10.305573	832.215616	11.126080
10.269661	831.545262	11.131098
10.382005	836.672877	11.136115
10.466684	834.318078	11.141133
10.521564	843.328229	11.146151
10.850368	855.135002	11.151168
10.348202	837.752596	11.156186
10.298489	847.794187	11.161203
10.626301	846.761652	11.166221
10.578891	854.270325	11.171239
10.167979	857.025274	11.176256
10.665391	851.440878	11.181274
10.983400	863.668320	11.186291
10.616791	855.070469	11.191309
10.602668	856.444823	11.196327
10.697108	864.478014	11.201344
10.545618	863.634682	11.206362
10.393951	863.697631	11.211379
10.723404	854.758940	11.216397
10.860617	859.815519	11.221415
10.839722	865.713592	11.226432
11.018638	856.027428	11.231450
10.583532	863.568416	11.236467
11.004750	860.926401	11.241485
10.899469	857.953876	11.246503
10.573706	853.124260	11.251520
10.903196	853.691361	11.256538
10.692003	858.848543	11.261555
10.673748	855.646658	11.266573
10.731794	849.025234	11.271591
10.334231	863.424600	11.276608
10.602245	854.512618	11.281626
10.747026	861.807590	11.286643
10.726198	859.635210	11.291661
10.876528	855.972361	11.296679
10.452161	868.276282	11.301696
10.725800	854.348670	11.306714
10.890923	858.548310	11.311731
10.314264	855.234571	11.316749
10.575325	851.439220	11.321767
10.422027	865.765466	11.326784
10.965870	878.434239	11.331802
11.224346	893.536770	11.336819
10.906386	886.762642	11.341837
10.887564	877.408799	11.346855
10.672948	893.488441	11.351872
11.029472	888.791885	11.356890
10.939000	893.021654	11.361907
10.944126	888.497847	11.366925
10.931503	896.841682	11.371943
10.642240	894.395653	11.376960
11.108470	887.933775	11.381978
10.766543	893.251586	11.386995
10.996604	892.762373	11.392013
11.083226	895.431006	11.397031
10.808677	888.537490	11.402048
10.914779	887.825115	11.407066
11.040066	901.071063	11.412083
10.894342	901.689693	11.417101
11.184756	896.765904	11.422119
10.947610	900.131031	11.427136
11.143083	897.549619	11.432154
11.145608	901.747063	11.437171
11.019703	896.239096	11.442189
10.941604	889.690196	11.447207
10.809672	899.690714	11.452224
11.229124	892.075221	11.457242
10.864250	904.115001	11.462259
10.960947	904.904108	11.467277
11.122312	901.732310	11.472295
10.976744	909.444262	11.477312
11.365140	916.695376	11.482330
11.098962	924.526909	11.487347
11.374079	921.745306	11.492365
11.663641	919.707731	11.497383
11.375555	904.321198	11.502400
11.446120	898.173246	11.507418
11.096949	902.354522	11.512435
11.018442	889.412309	11.517453
11.369977	882.076952	11.522471
11.305527	885.443399	11.527488
11.282221	883.202925	11.532506
10.886001	885.366894	11.537523
11.100467	903.727738	11.542541
11.637533	905.632448	11.547559
11.398724	913.109854	11.552576
11.388268	900.641379	11.557594
11.300026	902.448855	11.562611
11.293504	897.725803	11.567629
11.522690	909.081026	11.572647
11.705618	906.385554	11.577664
11.508154	889.144357	11.582682
11.416112	892.566159	11.587699
11.133515	888.943102	11.592717
11.421238	882.041125	11.597735
11.075879	896.064967	11.602752
11.323474	907.573825	11.607770
11.591133	916.092902	11.612787
11.433180	916.435618	11.617805
11.589895	923.497945	11.622823
11.386278	930.878198	11.627840
11.568406	915.689368	11.632858
11.706302	917.480659	11.637875
11.267278	921.392974	11.642893
11.541548	917.027337	11.647911
11.499909	926.309412	11.652928
11.534463	925.640377	11.657946
11.693019	912.384101	11.662963
11.768212	916.753365	11.667981
11.554452	918.466279	11.672999
11.535687	918.587531	11.678016
11.618557	916.106254	11.683034
11.512393	917.658445	11.688051
11.414814	927.237958	11.693069
11.804261	909.631849	11.698087
11.622158	917.562443	11.703104
11.249451	912.464217	11.708122
11.698859	912.689432	11.713139
11.601179	923.378354	11.718157
11.717466	914.884750	11.723175
11.527052	913.416001	11.728192
11.817810	916.578368	11.733210
11.683247	913.671307	11.738227
11.505490	927.127687	11.743245
11.936170	913.657853	11.748263
11.782852	915.264700	11.753280
11.607353	922.749736	11.758298
11.659811	922.682432	11.763315
11.629035	923.153294	11.768333
11.650970	919.295954	11.773351
11.710148	917.971299	11.778368
11.792665	912.198510	11.783386
11.716230	919.063627	11.788403
11.418912	916.709081	11.793421
11.808698	920.579425	11.798439
11.681690	942.878167	11.803456
11.884075	938.429550	11.808474
12.261573	953.270710	11.813491
11.831921	937.881601	11.818509
11.881354	928.055424	11.823527
12.082447	927.478885	11.828544
12.130698	924.542731	11.833562
12.230115	921.211510	11.838579
11.380964	920.892341	11.843597
11.846607	909.266631	11.848615
11.935253	926.718068	11.853632
11.857064	931.140686	11.858650
11.947318	942.011482	11.863667
11.858724	952.638293	11.868685
11.955553	935.700264	11.873703
11.998526	943.630214	11.878720
11.958946	945.011153	11.883738
11.955559	944.779089	11.888755
12.057203	955.603523	11.893773
12.312297	944.598844	11.898791
11.907872	953.135535	11.903808
12.089433	950.598541	11.908826
12.589076	952.161046	11.913843
12.434633	954.833388	11.918861
12.595426	938.824090	11.923879
12.290267	924.762741	11.928896
11.925290	915.919322	11.933914
12.194360	910.509717	11.938931
12.305349	917.055624	11.943949
12.057930	908.255338	11.948967
11.903900	910.301257	11.953984
11.904545	913.203803	11.959002
11.966294	921.688085	11.964019
11.914550	946.917928	11.969037
12.182449	954.437821	11.974055
12.285663	952.684631	11.979072
12.070636	953.130101	11.984090
12.641802	946.400047	11.989107
12.156194	952.047955	11.994125
12.375743	958.247178	11.999143
12.539328	948.207999	12.004160
12.276021	952.643955	12.009178
12.365179	945.095727	12.014195
11.966568	943.867346	12.019213
12.202532	947.504519	12.024231
12.443908	950.910886	12.029248
12.255264	945.484546	12.034266
12.662158	947.021859	12.039283
12.183736	951.343442	12.044301
12.285357	949.772397	12.049319
12.155069	953.136376	12.054336
12.281548	951.192334	12.059354
12.879120	951.306013	12.064371
12.193449	959.211356	12.069389
12.547911	946.170631	12.074407
12.640099	956.660821	12.079424
12.747425	955.371102	12.084442
12.535579	957.370304	12.089459
12.624930	956.542595	12.094477
12.735803	942.229277	12.099495
12.388109	941.301112	12.104512
12.285886	945.168292	12.109530
12.612639	946.701553	12.114547
12.402176	952.023204	12.119565
12.460936	944.957153	12.124583
12.446454	951.337245	12.129600
12.627502	953.403271	12.134618
12.457239	946.581039	12.139635
12.407554	954.666882	12.144653
12.561782	947.012214	12.149671
12.319960	951.403669	12.154688
12.348824	949.476185	12.159706
12.388273	942.029099	12.164723
12.301154	955.839376	12.169741
12.347639	963.229409	12.174759
12.527404	971.382379	12.179776
12.221188	961.470983	12.184794
12.591240	974.847717	12.189811
12.778277	978.038294	12.194829
12.915893	977.068346	12.199847
12.762758	974.571417	12.204864
12.876509	982.350303	12.209882
12.792862	971.457994	12.214899
12.480909	975.975236	12.219917
12.562836	971.735524	12.224935
12.989894	976.505968	12.229952
12.766204	971.591699	12.234970
13.313298	979.346068	12.239987
12.565893	987.721471	12.245005
12.572816	968.361788	12.250023
12.586736	978.879520	12.255040
12.724219	980.340980	12.260058
12.947973	977.301349	12.265075
13.114333	972.938212	12.270093
12.929039	970.721793	12.275111
13.103499	966.515577	12.280128
13.029168	972.742604	12.285146
12.896663	968.308883	12.290163
12.959271	970.711439	12.295181
12.838452	971.838129	12.300199
12.992804	971.645295	12.305216
12.896288	963.358942	12.310234
12.992293	966.155948	12.315251
13.057493	975.467603	12.320269
13.169601	971.074869	12.325287
13.099770	977.176355	12.330304
12.783430	970.810565	12.335322
13.206614	960.736265	12.340339
12.744776	970.205658	12.345357
13.259835	993.352834	12.350375
13.325130	981.165832	12.355392
13.064636	984.844279	12.360410
12.995243	967.652650	12.365427
13.085323	982.612688	12.370445
13.230075	993.778026	12.375463
13.609584	987.411961	12.380480
13.123740	978.752291	12.385498
13.470325	963.943644	12.390515
13.420266	964.309438	12.395533
13.131134	968.670150	12.400551
13.048383	961.836964	12.405568
13.059206	969.078187	12.410586
13.300383	970.874822	12.415603
12.942559	962.664415	12.420621
12.768319	980.352347	12.425639
13.200766	991.938135	12.430656
13.278650	998.287204	12.435674
13.198882	989.485094	12.440691
13.380224	1003.217495	12.445709
13.057175	994.905646	12.450727
13.135198	999.767750	12.455744
13.098207	999.457395	12.460762
13.359015	998.920176	12.465779
13.359392	998.721344	12.470797
13.343900	1001.532096	12.475815
13.766678	1004.823400	12.480832
13.323228	1003.323318	12.485850
13.178041	998.025191	12.490867
13.234896	1001.176703	12.495885
13.502861	993.620496	12.500903
13.296267	1005.509347	12.505920
13.363453	1001.294508	12.510938
13.478521	995.286781	12.515955
13.459441	1001.621594	12.520973
13.303723	1004.629967	12.525991
13.459728	1002.571587	12.531008
13.391339	1018.917684	12.536026
13.673905	1023.022334	12.541043
13.526011	1022.782702	12.546061
13.788912	1024.493467	12.551079
13.851191	1017.195314	12.556096
13.444951	1009.992068	12.561114
13.624086	998.066112	12.566131
13.740702	990.668033	12.571149
13.437046	993.448157	12.576167
13.740958	1011.743926	12.581184
13.756127	1022.918145	12.586202
13.987675	1013.171989	12.591219
13.767485	1001.357034	12.596237
13.388911	999.086399	12.601255
13.843589	996.115214	12.606272
13.679413	1002.058718	12.611290
13.592834	998.477583	12.616307
13.661687	1014.683632	12.621325
14.053080	1024.096807	12.626343
14.018734	1002.885726	12.631360
13.859455	1000.452406	12.636378
13.652720	988.968682	12.641395
13.840796	985.169637	12.646413
13.869535	987.894719	12.651431
13.852493	985.085502	12.656448
13.726998	992.977628	12.661466
14.052862	994.906300	12.666483
13.698065	990.073574	12.671501
13.882756	1013.712869	12.676519
14.143003	1003.829294	12.681536
13.663833	1012.783101	12.686554
13.892540	1023.276319	12.691571
14.052810	1026.548895	12.696589
13.954189	1029.100594	12.701607
13.833367	1022.899642	12.706624
13.875890	1028.963253	12.711642
13.934583	1013.393997	12.716659
14.046006	1032.031887	12.721677
14.317634	1024.346718	12.726695
14.253429	1021.922847	12.731712
14.346140	1030.985108	12.736730
14.476298	1010.082590	12.741747
13.979885	994.804081	12.746765
13.745797	1002.771672	12.751783
13.788354	995.078387	12.756800
13.935130	1019.432599	12.761818
14.328931	1018.823360	12.766835
14.118453	1012.053425	12.771853
13.887883	1024.254122	12.776871
14.074649	1025.626327	12.781888
14.004883	1019.198428	12.786906
14.184047	1025.077213	12.791923
14.007554	1024.184471	12.796941
14.353555	1019.189237	12.801959
14.434745	1021.803282	12.806976
14.124699	1025.976537	12.811994
14.014841	1020.375320	12.817011
13.996377	1028.326116	12.822029
14.128907	1014.029618	12.827047
14.215441	1021.295729	12.832064
14.413892	1021.538094	12.837082
14.049588	1022.184261	12.842099
14.350825	1019.675863	12.847117
14.062125	1024.653423	12.852135
14.444336	1017.700701	12.857152
14.027097	1016.960417	12.862170
14.241969	1028.656273	12.867187
14.575480	1042.583975	12.872205
14.130351	1047.129983	12.877223
14.398336	1044.644409	12.882240
14.439704	1055.963914	12.887258
14.171864	1052.602537	12.892275
14.654295	1052.205383	12.897293
14.727196	1060.685532	12.902311
14.675682	1052.420025	12.907328
14.786671	1059.286845	12.912346
14.439689	1046.117315	12.917363
14.423925	1041.372128	12.922381
14.673837	1049.378490	12.927399
14.367431	1051.860273	12.932416
14.545461	1054.359866	12.937434
14.778334	1057.904667	12.942451
14.777854	1054.862783	12.947469
14.690680	1050.586486	12.952487
14.608784	1024.929099	12.957504
14.689357	1028.159362	12.962522
14.593601	1026.370610	12.967539
14.601986	1032.843402	12.972557
14.488450	1050.662302	12.977575
14.808986	1046.003940	12.982592
14.850341	1054.474350	12.987610
14.763828	1050.792015	12.992627
14.886970	1048.805602	12.997645
14.689483	1061.874043	13.002663
14.716877	1044.007274	13.007680
14.516253	1046.529017	13.012698
14.965441	1042.638691	13.017715
15.155224	1037.209890	13.022733
14.793588	1038.594169	13.027751
15.139269	1031.534896	13.032768
14.992820	1026.872769	13.037786
14.547514	1013.516800	13.042803
14.698036	1022.635623	13.047821
14.710155	1042.255283	13.052839
14.932971	1039.367364	13.057856
14.915734	1035.897173	13.062874
14.655857	1045.009954	13.067891
15.106705	1042.110258	13.072909
15.147764	1048.160733	13.077927
15.087961	1051.178823	13.082944
15.158496	1053.045455	13.087962
14.968697	1056.695677	13.092979
14.947549	1043.214725	13.097997
14.892077	1049.550860	13.103015
15.194189	1046.355332	13.108032
14.976352	1041.171972	13.113050
15.006253	1049.467905	13.118067
15.227622	1037.934909	13.123085
14.961377	1050.640725	13.128103
15.071938	1046.681673	13.133120
15.168454	1042.649360	13.138138
15.112382	1040.013518	13.143155
15.220698	1036.907955	13.148173
14.972503	1051.904784	13.153191
15.140343	1044.665513	13.158208
15.116548	1034.558492	13.163226
14.932142	1047.566490	13.168243
15.172693	1034.698483	13.173261
15.011492	1037.726275	13.178279
15.028489	1038.482525	13.183296
15.052092	1046.120077	13.188314
15.005959	1042.768445	13.193331
15.224061	1033.954385	13.198349
15.133875	1046.035006	13.203367
15.204089	1051.257855	13.208384
15.373097	1059.459107	13.213402
15.333073	1061.829461	13.218419
15.632562	1068.985138	13.223437
15.340811	1067.426466	13.228455
15.320101	1053.601352	13.233472
15.581655	1063.094710	13.238490
15.228650	1060.961165	13.243507
15.416183	1057.667290	13.248525
15.714871	1064.442798	13.253543
15.380817	1062.598623	13.258560
15.641462	1061.674830	13.263578
15.158125	1063.870177	13.268595
15.565690	1059.938710	13.273613
15.588940	1061.419487	13.278631
15.430111	1060.215168	13.283648
15.403116	1062.606593	13.288666
15.364589	1066.853791	13.293683
16.003228	1060.537302	13.298701
15.905420	1066.317090	13.303719
15.860259	1060.216977	13.308736
16.050928	1050.579531	13.313754
15.702822	1046.439352	13.318771
15.890573	1031.025078	13.323789
15.512163	1038.059538	13.328807
15.372588	1035.092656	13.333824
15.670150	1032.418336	13.338842
15.393843	1030.407917	13.343859
15.606422	1046.217774	13.348877
15.869233	1058.586789	13.353895
16.002739	1055.880972	13.358912
15.742051	1046.458813	13.363930
15.667885	1059.765089	13.368947
15.751826	1067.135978	13.373965
15.646091	1061.022667	13.378983
15.674890	1064.295368	13.384000
15.890317	1071.010259	13.389018
15.697797	1060.931553	13.394035
15.990412	1058.742281	13.399053
16.034328	1072.575449	13.404071
15.648646	1062.899580	13.409088
15.869065	1064.281176	13.414106
15.815299	1069.307245	13.419123
16.017436	1059.823006	13.424141
16.331401	1067.038488	13.429159
16.107757	1069.376652	13.434176
15.965464	1063.833151	13.439194
16.224805	1069.349872	13.444211
16.102664	1060.047277	13.449229
16.102272	1065.157023	13.454247
15.902199	1063.973313	13.459264
16.054547	1060.446690	13.464282
15.978340	1064.095033	13.469299
16.328722	1052.467043	13.474317
15.869434	1065.709936	13.479335
15.873291	1062.470489	13.484352
16.073170	1061.508335	13.489370
15.955639	1068.168915	13.494387
16.160159	1058.262252	13.499405
16.079277	1071.223993	13.504423
15.916751	1060.641522	13.509440
16.108912	1069.779461	13.514458
16.016389	1062.771476	13.519475
16.171444	1052.593491	13.524493
15.990528	1065.729267	13.529511
15.854950	1068.817386	13.534528
16.098435	1079.553068	13.539546
15.879636	1094.948991	13.544563
16.127961	1087.834951	13.549581
16.386206	1090.869279	13.554599
16.445575	1095.312864	13.559616
16.487779	1096.122028	13.564634
16.423871	1096.115723	13.569651
16.598580	1093.451106	13.574669
16.808241	1094.560481	13.579687
16.060255	1093.593082	13.584704
16.688202	1082.445860	13.589722
16.410017	1097.939806	13.594739
16.415842	1089.805724	13.599757
16.561917	1100.884703	13.604775
16.596541	1097.561418	13.609792
16.506609	1093.639096	13.614810
16.273548	1101.321145	13.619827
16.661687	1094.956362	13.624845
16.503021	1092.864645	13.629863
16.770341	1094.262099	13.634880
16.690070	1099.287449	13.639898
16.504798	1096.712754	13.644915
16.569353	1085.648586	13.649933
16.687869	1093.223990	13.654951
16.305572	1091.166548	13.659968
16.927476	1093.319823	13.664986
16.518026	1095.430501	13.670003
16.534810	1090.134655	13.675021
16.693006	1094.001660	13.680039
16.670320	1086.676995	13.685056
16.815389	1088.443891	13.690074
16.808272	1083.664190	13.695091
16.526394	1090.411439	13.700109
16.660282	1094.774971	13.705127
16.656139	1095.369770	13.710144
16.912281	1091.074407	13.715162
16.565241	1096.790363	13.720179
16.739576	1108.396932	13.725197
16.878568	1106.622840	13.730215
16.896363	1114.136983	13.735232
17.438211	1106.912915	13.740250
16.850215	1100.662130	13.745267
17.047939	1084.799711	13.750285
17.049517	1086.925000	13.755303
16.781674	1077.825255	13.760320
17.425837	1074.302620	13.765338
16.770448	1088.250812	13.770355
16.941289	1080.609075	13.775373
17.183892	1084.715635	13.780391
17.147250	1081.962400	13.785408
17.382456	1081.660512	13.790426
16.832722	1085.006182	13.795443
16.789473	1081.426513	13.800461
17.116432	1099.554010	13.805479
17.184270	1112.839573	13.810496
17.198614	1109.647198	13.815514
17.347076	1114.877582	13.820531
16.882838	1102.151421	13.825549
16.976692	1103.110294	13.830567
17.061966	1113.882040	13.835584
17.354367	1108.512990	13.840602
17.293112	1116.915782	13.845619
17.207171	1106.627279	13.850637
17.264300	1113.509341	13.855655
17.161213	1119.319156	13.860672
17.768692	1119.746933	13.865690
17.443647	1111.258587	13.870707
17.452678	1117.391556	13.875725
17.446836	1105.899282	13.880743
17.104890	1117.281910	13.885760
17.144081	1107.995484	13.890778
17.369156	1114.756432	13.895795
17.242701	1112.306242	13.900813
17.550539	1111.916345	13.905831
17.245707	1121.885402	13.910848
17.496995	1115.064549	13.915866
17.633040	1116.162101	13.920883
17.074082	1119.777799	13.925901
17.187949	1109.218422	13.930919
17.194204	1111.907880	13.935936
17.255180	1106.586995	13.940954
17.441363	1104.068503	13.945971
17.604020	1113.289696	13.950989
17.552359	1124.049873	13.956007
17.731322	1133.108148	13.961024
17.867052	1127.988649	13.966042
17.694147	1120.060517	13.971059
17.436264	1108.298177	13.976077
17.945579	1122.320851	13.981095
17.535399	1122.983280	13.986112
17.961293	1122.208098	13.991130
17.518275	1123.540901	13.996147
18.014842	1128.194375	14.001165
17.983527	1113.544615	14.006183
17.789827	1112.262998	14.011200
17.628562	1101.041337	14.016218
17.701045	1114.939102	14.021235
17.772789	1124.857221	14.026253
18.137629	1132.761922	14.031271
17.887260	1124.593475	14.036288
18.032581	1099.524301	14.041306
17.913248	1096.163913	14.046323
18.015767	1103.437258	14.051341
18.090197	1096.536253	14.056359
17.884376	1100.551330	14.061376
17.674267	1102.459715	14.066394
18.016274	1115.318399	14.071411
17.963471	1125.576422	14.076429
18.132424	1133.228924	14.081447
18.138201	1137.916427	14.086464
18.243324	1131.364250	14.091482
18.287599	1120.112871	14.096499
18.036839	1103.293631	14.101517
18.172903	1101.494829	14.106535
18.125454	1101.090931	14.111552
18.152410	1092.175030	14.116570
18.263996	1090.492090	14.121587
17.814109	1100.638296	14.126605
18.314107	1114.118826	14.131623
18.041533	1131.625583	14.136640
18.472552	1124.360412	14.141658
18.645980	1115.032857	14.146675
18.211218	1109.910983	14.151693
18.314092	1088.599506	14.156711
18.036539	1106.955453	14.161728
18.073226	1099.552448	14.166746
17.747969	1115.925434	14.171763
18.121594	1130.281990	14.176781
18.288190	1116.962793	14.181799
18.161088	1127.922466	14.186816
18.504801	1123.537006	14.191834
18.580512	1137.962584	14.196851
18.514034	1128.143663	14.201869
18.692640	1133.282844	14.206887
18.378280	1126.450142	14.211904
18.371146	1133.171206	14.216922
18.274984	1130.399079	14.221939
18.368288	1131.872988	14.226957
18.690844	1127.352846	14.231975
18.639392	1140.344811	14.236992
18.716107	1132.850913	14.242010
18.457437	1129.609256	14.247027
18.618931	1130.076632	14.252045
18.803029	1126.576233	14.257063
18.672337	1137.874684	14.262080
18.517721	1133.150493	14.267098
18.717956	1124.003920	14.272115
18.570032	1131.134109	14.277133
18.748226	1126.378826	14.282151
18.680528	1138.487290	14.287168
18.725025	1135.186770	14.292186
18.763980	1125.302362	14.297203
18.666961	1127.335719	14.302221
18.812202	1126.931802	14.307239
18.572288	1129.693521	14.312256
18.638720	1131.723435	14.317274
18.865362	1125.275149	14.322291
18.976602	1126.985843	14.327309
19.027062	1125.487030	14.332327
18.690956	1133.754641	14.337344
18.889276	1132.927382	14.342362
19.002507	1127.795861	14.347379
18.777368	1142.911790	14.352397
19.253193	1137.244650	14.357415
18.823938	1141.943957	14.362432
18.963541	1139.563876	14.367450
19.259813	1156.065081	14.372467
19.288039	1148.094969	14.377485
19.164769	1131.254588	14.382503
19.304153	1126.976975	14.387520
19.157983	1124.435956	14.392538
19.080629	1124.400776	14.397555
18.919773	1120.526017	14.402573
19.230438	1120.956094	14.407591
19.005610	1126.995119	14.412608
19.069847	1137.132986	14.417626
19.270173	1149.204163	14.422643
19.049899	1148.343071	14.427661
19.110105	1153.113689	14.432679
19.000854	1151.687382	14.437696
18.907626	1152.118594	14.442714
19.398885	1146.333545	14.447731
19.301230	1147.736323	14.452749
19.260622	1150.034349	14.457767
19.194248	1156.631772	14.462784
19.226996	1149.777409	14.467802
19.273751	1149.112250	14.472819
19.018702	1149.305699	14.477837
19.490642	1141.558564	14.482855
19.253541	1158.224467	14.487872
19.429812	1151.602628	14.492890
19.512449	1167.965605	14.497907
19.377677	1172.696864	14.502925
19.575370	1175.371168	14.507943
19.527753	1185.102405	14.512960
19.633594	1179.374865	14.517978
20.040457	1170.469238	14.522995
19.479778	1156.282277	14.528013
19.774328	1144.795349	14.533031
19.568189	1145.464936	14.538048
19.540812	1150.026441	14.543066
19.571165	1147.120373	14.548083
19.037886	1163.134955	14.553101
19.542173	1161.516504	14.558119
19.886901	1172.489415	14.563136
19.856913	1178.140302	14.568154
20.023221	1175.140065	14.573171
19.914036	1178.394302	14.578189
20.040196	1179.172639	14.583207
19.732913	1178.188162	14.588224
19.625913	1167.931058	14.593242
20.023321	1172.713560	14.598259
19.574605	1177.571999	14.603277
19.832653	1173.901082	14.608295
19.958715	1177.377379	14.613312
19.741519	1176.950801	14.618330
20.037844	1181.261871	14.623347
19.754566	1181.835968	14.628365
20.163891	1175.573940	14.633383
20.080883	1177.730570	14.638400
20.190531	1178.030161	14.643418
19.588913	1176.785771	14.648435
19.705019	1171.761630	14.653453
20.018926	1180.031077	14.658471
20.122914	1177.111236	14.663488
20.323636	1184.123090	14.668506
20.438483	1176.863794	14.673523
20.000298	1180.744538	14.678541
20.322300	1178.024810	14.683559
20.174684	1178.629590	14.688576
20.237244	1175.371739	14.693594
20.286870	1168.125609	14.698611
20.294861	1183.802167	14.703629
20.476264	1172.911888	14.708647
19.975028	1173.837814	14.713664
19.937326	1172.689410	14.718682
20.349844	1165.096587	14.723699
20.230213	1172.065422	14.728717
20.264187	1174.828645	14.733735
20.132196	1176.300889	14.738752
20.303600	1184.067573	14.743770
20.409224	1194.925767	14.748787
20.572083	1199.383348	14.753805
20.576365	1198.688607	14.758823
21.036676	1200.280091	14.763840
20.570167	1179.184028	14.768858
20.967775	1169.961834	14.773875
20.941188	1167.908076	14.778893
20.754734	1157.555083	14.783911
21.046481	1164.342808	14.788928
20.620898	1160.920916	14.793946
20.726840	1168.428363	14.798963
20.254825	1173.208378	14.803981
20.508446	1165.090309	14.808999
20.904915	1167.154945	14.814016
20.392035	1167.235187	14.819034
20.893757	1155.166327	14.824051
20.561950	1168.706297	14.829069
20.676507	1159.974270	14.834087
20.865055	1157.064052	14.839104
20.607997	1160.298678	14.844122
20.925559	1165.263685	14.849139
20.659686	1155.081320	14.854157
20.959585	1159.717371	14.859175
20.747540	1160.726507	14.864192
20.581593	1166.156604	14.869210
20.977482	1161.768399	14.874227
20.643267	1164.614634	14.879245
20.906851	1185.706960	14.884263
20.919844	1187.111498	14.889280
20.870114	1193.031793	14.894298
21.272726	1195.669413	14.899315
20.968942	1197.030346	14.904333
20.784292	1192.548898	14.909351
21.156321	1194.035319	14.914368
21.118567	1187.546932	14.919386
20.988614	1192.623058	14.924403
21.063816	1199.534447	14.929421
20.859025	1193.060333	14.934439
20.973789	1197.082583	14.939456
20.886673	1196.220699	14.944474
21.242687	1187.228996	14.949491
21.111228	1197.774886	14.954509
21.027293	1186.992706	14.959527
21.364518	1198.184587	14.964544
21.412793	1196.172759	14.969562
21.224249	1190.896705	14.974579
21.176542	1192.477431	14.979597
21.170910	1193.735059	14.984615
21.144146	1199.280698	14.989632
21.312280	1218.377519	14.994650
21.494034	1223.531563	14.999667
21.694572	1223.173998	15.004685
21.278245	1230.906534	15.009703
21.689289	1215.671238	15.014720
21.577874	1219.433318	15.019738
22.007828	1219.851126	15.024755
21.713551	1202.660648	15.029773
21.586687	1191.582433	15.034791
21.497931	1190.973568	15.039808
21.323746	1198.046721	15.044826
21.651417	1193.434377	15.049843
21.586322	1214.029609	15.054861
21.873788	1221.567652	15.059879
22.191354	1216.331403	15.064896
21.721331	1196.730341	15.069914
21.651449	1186.966668	15.074931
21.569437	1178.690002	15.079949
21.695554	1187.184243	15.084967
21.642785	1190.059073	15.089984
21.821265	1211.011594	15.095002
22.072379	1212.114114	15.100019
22.029170	1216.441653	15.105037
21.859909	1201.390648	15.110055
21.835314	1187.395196	15.115072
21.625306	1211.134401	15.120090
21.936008	1212.790816	15.125107
21.908274	1212.793875	15.130125
21.581778	1215.416013	15.135143
22.152596	1209.581154	15.140160
22.123816	1220.093916	15.145178
22.141491	1217.591891	15.150195
22.370388	1221.440136	15.155213
22.245046	1206.143278	15.160231
22.307800	1206.099070	15.165248
22.215378	1216.462530	15.170266
22.334508	1205.583327	15.175283
22.217403	1190.555192	15.180301
22.178622	1182.115858	15.185319
22.196102	1176.722626	15.190336
21.968816	1182.337289	15.195354
22.033838	1198.617785	15.200371
22.013550	1210.287366	15.205389
21.937976	1209.785763	15.210407
22.216790	1207.485373	15.215424
21.940424	1216.703737	15.220442
22.435385	1214.886831	15.225459
22.362512	1213.797790	15.230477
21.919806	1217.510793	15.235495
22.407037	1203.817571	15.240512
22.493124	1215.911654	15.245530
22.439116	1206.000857	15.250547
22.189768	1211.256990	15.255565
22.324255	1223.963519	15.260583
22.738509	1218.211667	15.265600
22.405837	1225.088641	15.270618
22.644425	1236.566167	15.275635
22.509964	1237.953001	15.280653
22.531679	1242.717423	15.285671
22.808464	1241.261829	15.290688
22.614142	1245.695105	15.295706
22.444473	1238.275418	15.300723
22.420781	1242.991060	15.305741
22.461937	1240.291055	15.310759
22.927730	1246.971258	15.315776
23.034814	1245.102044	15.320794
22.741711	1234.735164	15.325811
22.822217	1245.086543	15.330829
22.845354	1236.859755	15.335847
22.804840	1232.320964	15.340864
22.741020	1245.244988	15.345882
22.658214	1236.895196	15.350899
22.962353	1234.155188	15.355917
22.970972	1243.781089	15.360935
23.256163	1234.371966	15.365952
22.877556	1239.131810	15.370970
23.308123	1237.988537	15.375987
22.704604	1240.564821	15.381005
22.594743	1236.233570	15.386023
23.070740	1237.334680	15.391040
22.669604	1237.980261	15.396058
22.978710	1227.077066	15.401075
23.026093	1232.473830	15.406093
22.697598	1249.914785	15.411111
23.409043	1258.910946	15.416128
23.354561	1265.335191	15.421146
23.251819	1260.417730	15.426163
23.631320	1256.327481	15.431181
23.481309	1254.818544	15.436199
23.198470	1227.624845	15.441216
23.271861	1232.501963	15.446234
23.301978	1240.790088	15.451251
23.279559	1233.377910	15.456269
23.151115	1260.708306	15.461287
23.460587	1260.408290	15.466304
23.502153	1251.669795	15.471322
23.683119	1252.283947	15.476339
23.739321	1258.980012	15.481357
23.812946	1250.115346	15.486375
23.709099	1231.572080	15.491392
23.608192	1224.191012	15.496410
23.673271	1221.900422	15.501427
23.604168	1230.716374	15.506445
23.829781	1222.013166	15.511463
24.086590	1218.316853	15.516480
23.552032	1218.397929	15.521498
23.852945	1227.242765	15.526515
23.896867	1220.989652	15.531533
23.476711	1224.315863	15.536551
23.600030	1227.489879	15.541568
23.484645	1227.703115	15.546586
23.185316	1223.900470	15.551603
23.518882	1227.254627	15.556621
23.718516	1250.264662	15.561639
23.866980	1254.864009	15.566656
23.844751	1258.956990	15.571674
24.011946	1262.905617	15.576691
24.085789	1255.305052	15.581709
24.128614	1259.002232	15.586727
24.002674	1247.794693	15.591744
24.119635	1242.754246	15.596762
23.866123	1239.014875	15.601779
23.933017	1240.029794	15.606797
24.120188	1252.918563	15.611815
24.281163	1246.849202	15.616832
24.034312	1252.460437	15.621850
23.869353	1242.683733	15.626867
24.199434	1247.813618	15.631885
23.890217	1248.153830	15.636903
24.075652	1252.197856	15.641920
23.850301	1254.238701	15.646938
23.914668	1247.927075	15.651955
24.102978	1250.163588	15.656973
23.970838	1250.901238	15.661991
24.083242	1251.490524	15.667008
24.111816	1257.656138	15.672026
24.301483	1273.455456	15.677043
24.445622	1276.959097	15.682061
24.573565	1287.154228	15.687079
24.585847	1283.261389	15.692096
24.333884	1280.680383	15.697114
24.553217	1277.987874	15.702131
24.767127	1282.556314	15.707149
24.533023	1286.063142	15.712167
24.542450	1266.098357	15.717184
24.548331	1266.804886	15.722202
24.510476	1272.579154	15.727219
24.836949	1267.559911	15.732237
24.447096	1286.166548	15.737255
24.863234	1278.843142	15.742272
24.928481	1284.584989	15.747290
24.661748	1267.407987	15.752307
24.589840	1256.887933	15.757325
24.683917	1280.783579	15.762343
24.736491	1279.271409	15.767360
24.674998	1275.600625	15.772378
24.490207	1282.482664	15.777395
24.736721	1281.955284	15.782413
24.698349	1292.977544	15.787431
25.002806	1280.197963	15.792448
24.856021	1289.419322	15.797466
24.469495	1278.760015	15.802483
24.682310	1281.799541	15.807501
24.884761	1285.242742	15.812519
24.985359	1274.714583	15.817536
24.819779	1285.957504	15.822554
25.168296	1296.306269	15.827571
25.287944	1300.582850	15.832589
25.278896	1290.759433	15.837607
25.186914	1280.374180	15.842624
25.361370	1280.974451	15.847642
25.484984	1268.404741	15.852659
25.663168	1278.973821	15.857677
25.326594	1278.049698	15.862695
25.104367	1276.947983	15.867712
24.956352	1275.920198	15.872730
25.040268	1274.093398	15.877747
25.501333	1273.285222	15.882765
25.136953	1277.837610	15.887783
25.173240	1275.185253	15.892800
25.615259	1278.373042	15.897818
25.198241	1293.512228	15.902835
25.612309	1291.239823	15.907853
25.058272	1289.909986	15.912871
25.423960	1299.105152	15.917888
25.508142	1310.263033	15.922906
25.259616	1308.847174	15.927923
25.569660	1305.455011	15.932941
25.501253	1310.983964	15.937959
25.381645	1304.844508	15.942976
25.476731	1303.943392	15.947994
25.513758	1309.095447	15.953011
25.851540	1295.869400	15.958029
25.914372	1309.414223	15.963047
25.569740	1306.673758	15.968064
25.753787	1300.710395	15.973082
25.691605	1311.789366	15.978099
25.914207	1303.508648	15.983117
25.815446	1304.030936	15.988135
25.501855	1307.169443	15.993152
25.891438	1304.066465	15.998170
25.501861	1302.489321	16.003187
25.924502	1306.033859	16.008205
26.033354	1328.262605	16.013223
26.114888	1323.989792	16.018240
26.060777	1319.652829	16.023258
26.060710	1321.083951	16.028275
26.232502	1312.653771	16.033293
26.160906	1312.177490	16.038311
25.934080	1318.680294	16.043328
26.295267	1310.153795	16.048346
26.204510	1322.454800	16.053363
26.637964	1315.674560	16.058381
25.931962	1310.952641	16.063399
26.387292	1314.694519	16.068416
26.462691	1311.430970	16.073434
26.251853	1320.163752	16.078451
26.107038	1320.659809	16.083469
26.311829	1319.923593	16.088487
26.328356	1309.918374	16.093504
26.410824	1309.649648	16.098522
26.036517	1319.357900	16.103539
26.528140	1317.195874	16.108557
26.461635	1315.700663	16.113575
26.902281	1307.268487	16.118592
26.666643	1315.965217	16.123610
26.650615	1317.355281	16.128627
26.588445	1317.259713	16.133645
26.503838	1316.735194	16.138663
26.174542	1312.112311	16.143680
26.528115	1310.023144	16.148698
26.298177	1316.459142	16.153715
26.421685	1314.888374	16.158733
26.439550	1313.692571	16.163751
26.330237	1321.278254	16.168768
26.707319	1331.063271	16.173786
26.829603	1341.227880	16.178803
27.117578	1354.703178	16.183821
26.950547	1342.959472	16.188839
27.133174	1350.306281	16.193856
27.048639	1327.999151	16.198874
27.026487	1322.093151	16.203891
26.774918	1313.490953	16.208909
26.667492	1316.303992	16.213927
27.168279	1334.047479	16.218944
27.425527	1326.186593	16.223962
26.677111	1321.655942	16.228979
26.624989	1322.590970	16.233997
26.941292	1332.987614	16.239015
26.671682	1339.289248	16.244032
27.367674	1329.649843	16.249050
27.290812	1345.120541	16.254067
27.363510	1336.706364	16.259085
27.315168	1346.895686	16.264103
27.077713	1340.495026	16.269120
27.337290	1331.018040	16.274138
27.251845	1338.456082	16.279155
27.213837	1324.382020	16.284173
27.305559	1336.866989	16.289191
27.291393	1328.742389	16.294208
27.156750	1335.818506	16.299226
27.066419	1344.921890	16.304243
27.464129	1333.973241	16.309261
27.304532	1343.796740	16.314279
27.629444	1356.450587	16.319296
28.074903	1357.943370	16.324314
27.735416	1348.994300	16.329331
27.954121	1336.422569	16.334349
27.868310	1339.952491	16.339367
27.311000	1338.151154	16.344384
27.750216	1331.889627	16.349402
27.641950	1341.392033	16.354419
27.781366	1334.207728	16.359437
27.914457	1330.867300	16.364455
27.751909	1335.281167	16.369472
27.813249	1328.457423	16.374490
27.621300	1323.549202	16.379507
27.657710	1340.473153	16.384525
27.989443	1358.731264	16.389543
28.120109	1365.759526	16.394560
28.050637	1365.570287	16.399578
27.837818	1361.683993	16.404595
28.006141	1360.424297	16.409613
27.890917	1367.402333	16.414631
28.083333	1355.775472	16.419648
28.122491	1358.655584	16.424666
27.914727	1361.770673	16.429683
28.014413	1353.266193	16.434701
28.229368	1357.531338	16.439719
27.923559	1361.304382	16.444736
28.139887	1353.289238	16.449754
28.125613	1359.035225	16.454771
28.324898	1361.225844	16.459789
28.364311	1351.287673	16.464807
28.324738	1358.389789	16.469824
28.467587	1346.323121	16.474842
28.337563	1355.962207	16.479859
28.150817	1347.951212	16.484877
28.383245	1356.980294	16.489895
28.100792	1352.775618	16.494912
28.526448	1376.623987	16.499930
28.617839	1374.630981	16.504947
28.680605	1384.134620	16.509965
29.239002	1378.030502	16.514983
28.373200	1369.022116	16.520000
28.849992	1346.312963	16.525018
28.862936	1355.441772	16.530035
28.781256	1339.006473	16.535053
29.048546	1344.303479	16.540071
28.585180	1348.054577	16.545088
28.711916	1346.058084	16.550106
28.952026	1339.623227	16.555123
28.816396	1339.906351	16.560141
28.893830	1349.178805	16.565159
28.511330	1345.154867	16.570176
28.674489	1337.696161	16.575194
28.651311	1359.163367	16.580211
28.658014	1371.373864	16.585229
29.013507	1373.396496	16.590247
29.081051	1374.386120	16.595264
29.209837	1371.516073	16.600282
28.976367	1380.747115	16.605299
29.007109	1384.267196	16.610317
28.791170	1380.643613	16.615335
28.886899	1375.901909	16.620352
29.188340	1368.023843	16.625370
29.189094	1380.642411	16.630387
29.265263	1384.819130	16.635405
29.407477	1368.296335	16.640423
29.486454	1377.463827	16.645440
29.268307	1365.391566	16.650458
29.216413	1376.817299	16.655475
29.451525	1373.813899	16.660493
29.227797	1370.834903	16.665511
29.391706	1367.340155	16.670528
29.440350	1370.191927	16.675546
29.413223	1371.185810	16.680563
29.348419	1368.703717	16.685581
29.307801	1373.882823	16.690599
29.385678	1398.741946	16.695616
29.706217	1399.221184	16.700634
29.682067	1404.311354	16.705651
29.705701	1390.550642	16.710669
29.970713	1391.332376	16.715687
29.621993	1409.115829	16.720704
29.879074	1386.852440	16.725722
29.735862	1398.302757	16.730739
29.924403	1395.737766	16.735757
29.829422	1390.209540	16.740775
29.742291	1394.462514	16.745792
30.013892	1394.186090	16.750810
29.806970	1396.342797	16.755827
29.673201	1389.023389	16.760845
30.089747	1392.893754	16.765863
29.923167	1395.442986	16.770880
29.798982	1385.076773	16.775898
29.909657	1393.710297	16.780915
29.825253	1392.876297	16.785933
29.881781	1394.300810	16.790951
30.009636	1404.315328	16.795968
30.263774	1422.211173	16.800986
30.350984	1423.367620	16.806003
30.423568	1430.108289	16.811021
30.551044	1418.704730	16.816039
30.397612	1419.182531	16.821056
30.622257	1413.234843	16.826074
30.402303	1391.466571	16.831091
30.167811	1388.537778	16.836109
30.582874	1396.889016	16.841127
30.398823	1408.378387	16.846144
30.921488	1412.435118	16.851162
30.575248	1402.233614	16.856179
30.596279	1382.536437	16.861197
30.418820	1374.473891	16.866215
29.964323	1397.933006	16.871232
30.387845	1406.215526	16.876250
30.646222	1420.558761	16.881267
30.510188	1418.900646	16.886285
30.849600	1412.781595	16.891303
30.807201	1423.846347	16.896320
30.942131	1415.812366	16.901338
30.976576	1420.096002	16.906355
30.591269	1417.769333	16.911373
31.181383	1415.574057	16.916391
30.881807	1421.050778	16.921408
31.254049	1415.234946	16.926426
31.022179	1419.488272	16.931443
30.480071	1420.774514	16.936461
30.838207	1412.105555	16.941479
30.696600	1410.603873	16.946496
30.887858	1409.341950	16.951514
30.525030	1414.711822	16.956531
30.942203	1430.386623	16.961549
31.415338	1427.889854	16.966567
31.439208	1438.634200	16.971584
31.258371	1444.934956	16.976602
31.748535	1436.081525	16.981619
31.193584	1428.455075	16.986637
31.400811	1408.417984	16.991655
30.991043	1408.407137	16.996672
31.324468	1412.955039	17.001690
31.600782	1418.610806	17.006707
31.278003	1430.235760	17.011725
31.576629	1426.309249	17.016743
31.491572	1426.780847	17.021760
31.307706	1426.513307	17.026778
31.688271	1413.508026	17.031795
31.669208	1417.583202	17.036813
31.763442	1424.991139	17.041831
31.793932	1426.342803	17.046848
31.574336	1419.967892	17.051866
31.593972	1425.652384	17.056883
31.772205	1426.276839	17.061901
31.906104	1417.893821	17.066919
31.770747	1426.364168	17.071936
31.541561	1423.363232	17.076954
31.825945	1424.440968	17.081971
31.647127	1426.724912	17.086989
31.857686	1416.940248	17.092007
31.748733	1423.017284	17.097024
31.871226	1415.660156	17.102042
32.100973	1427.802270	17.107059
31.888291	1434.857889	17.112077
32.225622	1426.796294	17.117095
32.138020	1432.717834	17.122112
32.035848	1435.852854	17.127130
32.341878	1451.628362	17.132147
32.290243	1454.055029	17.137165
32.496846	1451.540974	17.142183
32.104226	1441.163661	17.147200
32.022606	1434.832826	17.152218
32.308583	1449.118368	17.157235
32.426916	1454.438895	17.162253
32.499567	1445.142790	17.167271
32.489990	1454.289165	17.172288
32.265235	1460.827905	17.177306
32.144838	1457.470370	17.182323
32.475986	1452.084158	17.187341
32.540371	1450.211753	17.192359
32.700426	1449.054993	17.197376
32.805002	1456.095490	17.202394
33.033774	1444.535770	17.207411
32.776231	1454.214536	17.212429
33.041809	1450.958443	17.217447
32.880066	1448.088457	17.222464
32.485528	1456.871419	17.227482
32.925863	1452.440341	17.232499
32.623248	1459.648657	17.237517
32.860393	1444.327761	17.242535
32.926356	1447.076287	17.247552
32.727509	1457.074858	17.252570
33.045919	1452.820267	17.257587
32.792105	1456.211500	17.262605
32.529061	1441.395865	17.267623
32.808116	1452.781814	17.272640
32.728840	1456.925631	17.277658
32.935557	1460.295726	17.282675
32.880211	1475.356305	17.287693
33.100554	1478.162343	17.292711
33.096048	1486.957115	17.297728
32.906450	1477.841027	17.302746
33.425954	1479.367624	17.307763
33.306099	1482.835499	17.312781
33.383171	1473.854388	17.317799
33.239760	1477.313564	17.322816
33.146241	1473.712995	17.327834
33.356657	1474.665977	17.332851
33.284782	1472.377556	17.337869
33.498271	1472.499724	17.342887
33.417972	1496.361586	17.347904
33.648637	1495.961626	17.352922
34.289794	1498.684603	17.357939
33.889176	1485.437357	17.362957
33.897033	1467.212316	17.367975
33.858699	1466.060058	17.372992
33.804900	1463.477704	17.378010
33.985418	1461.280167	17.383027
34.133833	1463.418989	17.388045
34.160842	1471.002644	17.393063
33.861224	1461.551638	17.398080
34.360861	1463.220891	17.403098
34.392850	1449.233549	17.408115
34.142424	1462.151646	17.413133
33.669041	1465.120977	17.418151
33.839002	1465.852313	17.423168
33.799033	1467.815245	17.428186
33.894303	1458.992545	17.433203
33.978810	1453.726698	17.438221
33.860031	1456.521171	17.443239
33.698465	1461.350653	17.448256
34.199782	1489.480706	17.453274
34.576889	1487.141166	17.458291
34.499831	1494.617263	17.463309
34.520049	1492.408077	17.468327
34.603504	1495.749771	17.473344
34.412453	1472.575434	17.478362
34.865091	1467.681298	17.483379
34.069866	1463.577639	17.488397
34.321641	1467.530818	17.493415
34.794453	1486.895234	17.498432
34.658747	1484.735489	17.503450
34.754239	1484.502397	17.508467
34.711293	1491.932294	17.513485
34.953528	1486.434810	17.518503
34.631914	1474.609908	17.523520
34.289117	1461.729482	17.528538
34.930620	1477.638442	17.533555
34.403953	1486.112593	17.538573
34.574680	1484.726901	17.543591
34.878585	1490.023799	17.548608
34.495967	1491.258441	17.553626
34.939878	1492.892832	17.558643
34.952148	1497.626612	17.563661
35.028232	1493.010959	17.568679
34.681575	1491.716842	17.573696
34.873141	1491.588707	17.578714
35.114930	1481.987410	17.583731
34.858703	1492.536050	17.588749
34.984327	1512.313493	17.593767
35.627133	1525.932548	17.598784
35.159688	1531.056793	17.603802
35.394818	1519.749899	17.608819
35.100625	1524.390340	17.613837
35.141105	1522.720309	17.618855
35.524696	1514.385657	17.623872
35.354937	1520.149969	17.628890
35.591232	1514.092047	17.633907
35.719052	1518.111433	17.638925
35.511454	1512.673070	17.643943
35.969510	1514.555905	17.648960
35.750629	1510.276487	17.653978
35.705343	1503.081742	17.658995
35.913936	1508.714898	17.664013
35.929364	1503.881728	17.669031
36.185754	1483.315540	17.674048
35.607910	1487.721052	17.679066
35.831754	1475.666068	17.684083
35.736285	1483.941655	17.689101
35.921600	1483.405899	17.694119
35.890524	1465.837297	17.699136
35.448136	1484.314289	17.704154
35.740227	1493.489082	17.709171
36.103708	1498.094631	17.714189
35.592969	1501.872507	17.719207
36.219261	1494.935064	17.724224
35.967115	1509.179847	17.729242
36.144567	1498.564795	17.734259
36.176196	1510.622851	17.739277
36.378542	1506.596516	17.744295
36.392538	1497.239620	17.749312
35.639528	1505.665435	17.754330
35.807353	1496.884242	17.759347
36.012844	1511.042226	17.764365
36.172698	1526.453043	17.769383
36.313617	1530.387980	17.774400
36.373698	1537.589818	17.779418
36.712219	1528.376015	17.784435
36.468119	1531.704239	17.789453
36.355454	1528.419817	17.794471
36.596992	1528.764505	17.799488
36.726025	1533.177785	17.804506
36.868084	1530.287400	17.809523
36.446239	1531.340747	17.814541
36.485957	1528.594473	17.819559
36.642467	1531.538649	17.824576
36.688277	1531.037015	17.829594
37.139353	1544.775629	17.834611
37.086255	1536.346740	17.839629
36.659924	1530.490656	17.844647
37.167194	1533.995645	17.849664
36.893032	1558.007024	17.854682
37.176097	1552.490945	17.859699
37.251840	1556.681955	17.864717
37.448707	1551.397077	17.869735
37.387182	1533.422420	17.874752
37.004554	1519.682013	17.879770
37.340957	1515.911428	17.884787
36.896126	1522.465375	17.889805
37.523818	1529.032676	17.894823
37.686955	1531.819851	17.899840
37.020162	1529.458671	17.904858
37.261977	1530.022603	17.909875
37.358603	1545.923826	17.914893
37.224094	1554.697643	17.919911
37.386981	1547.982971	17.924928
37.444597	1550.631324	17.929946
37.818291	1544.868353	17.934963
37.749621	1547.921078	17.939981
37.457787	1543.562392	17.944999
37.834873	1548.916090	17.950016
37.437201	1554.780358	17.955034
37.641959	1550.288656	17.960051
37.780364	1549.747673	17.965069
37.741990	1552.798925	17.970087
37.771875	1542.000012	17.975104
37.494203	1547.103862	17.980122
37.604650	1548.758042	17.985139
37.809633	1564.327565	17.990157
38.076879	1577.363581	17.995175
38.216794	1581.228226	18.000192
37.923147	1583.440656	18.005210
38.284760	1566.657306	18.010227
38.354531	1576.072896	18.015245
38.333199	1573.065859	18.020263
38.321265	1568.888376	18.025280
38.119351	1570.453730	18.030298
38.521206	1568.882910	18.035315
38.642913	1567.824223	18.040333
38.321685	1569.428230	18.045351
38.371319	1568.870844	18.050368
38.208306	1564.728614	18.055386
38.043567	1574.996808	18.060403
38.412937	1574.830964	18.065421
38.453457	1570.230625	18.070439
38.831822	1567.276697	18.075456
38.593019	1571.500109	18.080474
38.631558	1570.857552	18.085491
38.399762	1572.115651	18.090509
38.465292	1574.568998	18.095527
38.648003	1589.457593	18.100544
38.573796	1599.624593	18.105562
39.048576	1600.087748	18.110579
38.924185	1607.235912	18.115597
38.715729	1607.554720	18.120615
39.050723	1595.085571	18.125632
38.867382	1599.110045	18.130650
38.788454	1600.492046	18.135667
39.152896	1595.682552	18.140685
39.079642	1602.172250	18.145703
39.294889	1593.267403	18.150720
39.138695	1596.005891	18.155738
39.247445	1582.064380	18.160755
39.592912	1586.560734	18.165773
39.492269	1587.691607	18.170791
39.445295	1585.601799	18.175808
39.416458	1591.097136	18.180826
39.562786	1590.986333	18.185843
39.609644	1583.159368	18.190861
39.730003	1594.663038	18.195879
39.652194	1587.653166	18.200896
39.416663	1579.903670	18.205914
39.676233	1587.042184	18.210931
39.712486	1586.676775	18.215949
39.515661	1583.079507	18.220967
39.627688	1581.705100	18.225984
39.744654	1601.855744	18.231002
39.637085	1617.623136	18.236019
40.110873	1620.231724	18.241037
39.820402	1626.232991	18.246055
39.966572	1615.522252	18.251072
39.961775	1616.790012	18.256090
39.744213	1615.921356	18.261107
39.880256	1619.281535	18.266125
39.726557	1609.312971	18.271143
39.731967	1614.558157	18.276160
39.986562	1617.121543	18.281178
40.124983	1617.834094	18.286195
40.248411	1611.937343	18.291213
40.112825	1629.353080	18.296231
40.594230	1632.215920	18.301248
40.758299	1627.540382	18.306266
40.587168	1611.468030	18.311283
40.822520	1599.517343	18.316301
40.612800	1603.023353	18.321319
40.519484	1600.701455	18.326336
40.557374	1599.769242	18.331354
40.884182	1593.652208	18.336371
40.851188	1593.970702	18.341389
40.672189	1600.338933	18.346407
41.100959	1599.436879	18.351424
40.865018	1605.375172	18.356442
40.637697	1596.979035	18.361459
40.932783	1600.035318	18.366477
41.030243	1607.346353	18.371495
41.002339	1594.532177	18.376512
40.969596	1597.020304	18.381530
40.869505	1597.311720	18.386547
41.065698	1593.372208	18.391565
40.718543	1600.783238	18.396583
41.201126	1601.863603	18.401600
41.128391	1617.130347	18.406618
41.159893	1625.557426	18.411635
41.148886	1613.599883	18.416653
41.048638	1618.593670	18.421671
41.294302	1619.709328	18.426688
41.215262	1626.039758	18.431706
41.176096	1617.220724	18.436723
41.400375	1612.804511	18.441741
41.004551	1626.057054	18.446759
41.195030	1627.906258	18.451776
41.489125	1633.421365	18.456794
41.580468	1650.318843	18.461811
41.732236	1649.299267	18.466829
41.771674	1646.341602	18.471847
42.008826	1649.835439	18.476864
42.036286	1644.305747	18.481882
41.699800	1652.123301	18.486899
41.958001	1642.533755	18.491917
41.579123	1645.090227	18.496935
41.599944	1641.967929	18.501952
41.524005	1636.905359	18.506970
41.679218	1633.216717	18.511987
42.280620	1633.104972	18.517005
42.067518	1640.138706	18.522023
42.295576	1642.111610	18.527040
42.285971	1640.461670	18.532058
41.988243	1641.515338	18.537075
42.416048	1647.499254	18.542093
42.058025	1657.983365	18.547111
42.130020	1663.712818	18.552128
42.486321	1674.436141	18.557146
42.373209	1666.404520	18.562163
42.229359	1670.198851	18.567181
42.394631	1669.440817	18.572199
42.392885	1660.663987	18.577216
42.187447	1656.723246	18.582234
42.185060	1661.351236	18.587251
42.791922	1674.008266	18.592269
42.631277	1689.542000	18.597287
43.052761	1688.849021	18.602304
43.239650	1690.084260	18.607322
42.870621	1673.570595	18.612339
42.965862	1664.161562	18.617357
42.749699	1660.211966	18.622375
43.073054	1670.809246	18.627392
43.342639	1679.356774	18.632410
43.292303	1668.972631	18.637427
43.343588	1660.177572	18.642445
42.990102	1653.583789	18.647463
43.134203	1648.882024	18.652480
43.251641	1653.338990	18.657498
43.341550	1658.702877	18.662515
43.295557	1651.619204	18.667533
43.199242	1660.215497	18.672551
43.167835	1674.065613	18.677568
43.268811	1677.007202	18.682586
43.441504	1682.857784	18.687603
43.870049	1675.931352	18.692621
43.355508	1678.740607	18.697639
43.472016	1680.781987	18.702656
43.903270	1684.416527	18.707674
43.756018	1682.844099	18.712691
43.722828	1680.906721	18.717709
43.098696	1680.176248	18.722727
43.465204	1682.770721	18.727744
43.753086	1690.373887	18.732762
43.760593	1706.787670	18.737779
44.411043	1698.996531	18.742797
43.976039	1705.933966	18.747815
44.241204	1709.704676	18.752832
43.995240	1713.928524	18.757850
43.633762	1717.848272	18.762867
44.361043	1701.710136	18.767885
43.885913	1710.789655	18.772903
44.564403	1711.516723	18.777920
44.696448	1703.725592	18.782938
44.555944	1704.678820	18.787955
44.542948	1702.429828	18.792973
44.486463	1699.766382	18.797991
44.413656	1697.926114	18.803008
44.629391	1702.317999	18.808026
44.591792	1701.323476	18.813043
44.665368	1697.327864	18.818061
44.575611	1701.086080	18.823079
44.872465	1701.154684	18.828096
44.860353	1699.477987	18.833114
44.823226	1702.231818	18.838131
44.877667	1690.249993	18.843149
45.052300	1701.451842	18.848167
44.960438	1705.211195	18.853184
44.958099	1697.970272	18.858202
44.998975	1704.629304	18.863219
45.169100	1693.971631	18.868237
44.849555	1697.789154	18.873255
45.012311	1700.845321	18.878272
45.087531	1704.877796	18.883290
44.673502	1702.028277	18.888307
45.003181	1706.235548	18.893325
45.123128	1722.514194	18.898343
45.144111	1732.217486	18.903360
45.252130	1723.212997	18.908378
45.206061	1727.082489	18.913395
45.328560	1721.323252	18.918413
45.503516	1729.804981	18.923431
45.453358	1730.306636	18.928448
45.525992	1722.637144	18.933466
45.068028	1723.235851	18.938483
45.117633	1734.520631	18.943501
45.282438	1752.324958	18.948519
45.331637	1753.067643	18.953536
45.666266	1747.227602	18.958554
45.941175	1755.685315	18.963571
45.900132	1744.925170	18.968589
46.365034	1740.940735	18.973607
46.176021	1735.058663	18.978624
46.547345	1741.204331	18.983642
46.376276	1745.111455	18.988659
46.227052	1735.366084	18.993677
46.419802	1742.710224	18.998695
46.449987	1731.457978	19.003712
46.762984	1742.777498	19.008730
46.457725	1742.158396	19.013747
46.442930	1739.764420	19.018765
46.684722	1739.427573	19.023783
46.639289	1736.275281	19.028800
46.699694	1738.528715	19.033818
46.451706	1734.337517	19.038835
46.881258	1729.085705	19.043853
46.586459	1738.120026	19.048871
46.660089	1734.362979	19.053888
47.060187	1732.934955	19.058906
46.813645	1741.534514	19.063923
46.902394	1735.908419	19.068941
46.821357	1734.739984	19.073959
46.362847	1734.248620	19.078976
46.780279	1730.464174	19.083994
46.288018	1736.162674	19.089011
46.786303	1748.542861	19.094029
46.995522	1762.493765	19.099047
46.860953	1766.246424	19.104064
47.198725	1762.661776	19.109082
46.950748	1767.697000	19.114099
47.407218	1765.336406	19.119117
47.282458	1761.558264	19.124135
47.095354	1776.690164	19.129152
47.275971	1770.859474	19.134170
47.319820	1788.634264	19.139187
47.629743	1786.123127	19.144205
47.701375	1791.450323	19.149223
47.850332	1787.046927	19.154240
48.003035	1779.837774	19.159258
47.668599	1787.720018	19.164275
48.046999	1792.074758	19.169293
48.220224	1790.750831	19.174311
48.025896	1784.948361	19.179328
48.228627	1756.133160	19.184346
47.791194	1764.184809	19.189363
47.651543	1757.148092	19.194381
47.726021	1763.900011	19.199399
48.379769	1775.680459	19.204416
48.303858	1772.802500	19.209434
48.098178	1785.475659	19.214451
48.112811	1776.428727	19.219469
48.341592	1777.956250	19.224487
47.873154	1780.068908	19.229504
48.648325	1787.988290	19.234522
48.102546	1788.375948	19.239539
47.961966	1785.934288	19.244557
48.166332	1781.736681	19.249575
48.354021	1805.359368	19.254592
48.240152	1810.899570	19.259610
48.498553	1813.772598	19.264627
48.475560	1812.324859	19.269645
48.539423	1811.251717	19.274663
48.437301	1813.658452	19.279680
48.595506	1810.227937	19.284698
48.730954	1827.250984	19.289715
48.848721	1838.228093	19.294733
49.265329	1839.208375	19.299751
49.441731	1841.360726	19.304768
49.723641	1827.106856	19.309786
49.572232	1814.292871	19.314803
49.522990	1803.841132	19.319821
49.690111	1806.028480	19.324839
48.965515	1810.523340	19.329856
49.398464	1793.120450	19.334874
49.293908	1800.807942	19.339891
49.065055	1794.396613	19.344909
49.665321	1801.145741	19.349927
49.461281	1798.898446	19.354944
49.575172	1796.941818	19.359962
49.735030	1800.890618	19.364979
49.478433	1800.172510	19.369997
49.362851	1794.281406	19.375015
49.520789	1818.671250	19.380032
49.667563	1818.535176	19.385050
49.188828	1821.897982	19.390067
49.608080	1818.554162	19.395085
49.860586	1817.611204	19.400103
49.506287	1836.455133	19.405120
49.824361	1835.628090	19.410138
50.178915	1851.892829	19.415155
50.147510	1856.494186	19.420173
50.509093	1853.183924	19.425191
50.367397	1860.080736	19.430208
50.504851	1846.970465	19.435226
50.423535	1858.017167	19.440243
50.366276	1853.336083	19.445261
50.879544	1843.352602	19.450279
51.010334	1855.642148	19.455296
51.081817	1843.981797	19.460314
50.756930	1848.225048	19.465331
50.976983	1833.334951	19.470349
50.937601	1819.418936	19.475367
50.479740	1822.708205	19.480384
50.815582	1825.566051	19.485402
51.007797	1837.553678	19.490419
50.780281	1841.544976	19.495437
51.148813	1848.430528	19.500455
50.964275	1848.510731	19.505472
51.186966	1849.708165	19.510490
51.238506	1843.080701	19.515507
51.076260	1845.726533	19.520525
51.007508	1845.069052	19.525543
50.866496	1845.828671	19.530560
50.900326	1854.557854	19.535578
51.063671	1850.355997	19.540595
51.015695	1852.649441	19.545613
51.101013	1858.600779	19.550631
51.057548	1872.867641	19.555648
51.419748	1883.608637	19.560666
51.426938	1877.551108	19.565683
51.311134	1876.777400	19.570701
51.616674	1873.904766	19.575719
51.602835	1887.595075	19.580736
52.003194	1897.904560	19.585754
51.981589	1903.278335	19.590771
52.021930	1894.810157	19.595789
52.497457	1890.692821	19.600807
52.105472	1879.280840	19.605824
52.261816	1868.472178	19.610842
52.375795	1858.096134	19.615859
51.960057	1860.678428	19.620877
52.664777	1851.360887	19.625895
52.176393	1861.359626	19.630912
52.133195	1853.863188	19.635930
52.506385	1854.651053	19.640947
52.589355	1861.291765	19.645965
52.735798	1852.416273	19.650983
52.241980	1862.996628	19.656000
52.182125	1854.916327	19.661018
52.499593	1880.516876	19.666035
52.501253	1880.926883	19.671053
52.957594	1891.215678	19.676071
52.805334	1890.525172	19.681088
52.902486	1891.617016	19.686106
53.218466	1890.147000	19.691123
52.862763	1894.212687	19.696141
53.001370	1886.051082	19.701159
52.588975	1879.420892	19.706176
52.627767	1894.658813	19.711194
52.712693	1887.816350	19.716211
52.803518	1897.858973	19.721229
53.247525	1907.071459	19.726247
53.164510	1915.271984	19.731264
53.369464	1915.614472	19.736282
53.455062	1909.666391	19.741299
53.274735	1914.839676	19.746317
53.573471	1918.774960	19.751335
53.548272	1914.291308	19.756352
53.560455	1914.059013	19.761370
53.773773	1907.466940	19.766387
53.627103	1909.780671	19.771405
53.716135	1905.005663	19.776423
53.364383	1914.241644	19.781440
53.778946	1934.595811	19.786458
54.366864	1934.895362	19.791475
53.977427	1944.801392	19.796493
54.338229	1943.324344	19.801511
54.428793	1936.866760	19.806528
54.162952	1931.334347	19.811546
54.205524	1927.776887	19.816563
54.483370	1931.805005	19.821581
54.522236	1936.412467	19.826599
54.802430	1935.290898	19.831616
54.562817	1930.506912	19.836634
54.191590	1916.645363	19.841651
54.438213	1916.656537	19.846669
54.406400	1923.787549	19.851687
54.084259	1933.743847	19.856704
54.099961	1934.236178	19.861722
54.212034	1935.357445	19.866739
54.522543	1940.585295	19.871757
55.031199	1953.548192	19.876775
54.767354	1954.554930	19.881792
54.568072	1947.639813	19.886810
55.294535	1946.838452	19.891827
54.808535	1955.764004	19.896845
54.979111	1947.943536	19.901863
55.169135	1949.549543	19.906880
55.027048	1944.599795	19.911898
54.806465	1957.525171	19.916915
54.829520	1968.554670	19.921933
55.561858	1977.981666	19.926951
55.633143	1982.244791	19.931968
55.665685	1975.394428	19.936986
55.508081	1976.100893	19.942003
55.583625	1981.564123	19.947021
55.752899	1979.542395	19.952039
55.504903	1977.256288	19.957056
55.559988	1979.605128	19.962074
55.820530	1974.150900	19.967091
55.672442	1981.480328	19.972109
55.811986	1970.309016	19.977127
55.622881	1976.982622	19.982144
55.792685	1981.809760	19.987162
56.148318	1982.751723	19.992179
55.955192	1996.472995	19.997197
56.012548	1993.787893	20.002215
56.232535	1995.903916	20.007232
56.221565	1988.989490	20.012250
56.533102	1992.346677	20.017267
56.280961	1993.468411	20.022285
56.327520	2001.085310	20.027303
56.608215	1991.239852	20.032320
56.449418	1996.621808	20.037338
56.570744	1994.883614	20.042355
56.365554	1996.598374	20.047373
56.662324	2009.896408	20.052391
56.698750	2016.926792	20.057408
56.689685	2015.094828	20.062426
57.075715	2025.773710	20.067443
56.921044	2031.279407	20.072461
57.080341	2012.816439	20.077479
57.398192	2024.144417	20.082496
57.296661	2021.821453	20.087514
57.521121	2013.975888	20.092531
57.296306	2027.570148	20.097549
57.640924	2007.586704	20.102567
57.623472	2007.943185	20.107584
57.189147	2018.262608	20.112602
57.746594	2003.538535	20.117619
57.450752	2010.618420	20.122637
57.606775	2008.913063	20.127655
58.006546	2006.425599	20.132672
57.866238	2016.629014	20.137690
57.813017	2002.637959	20.142707
57.908107	2003.990787	20.147725
57.909541	2003.467351	20.152743
57.676225	1999.016954	20.157760
57.690723	2005.478903	20.162778
57.791512	1995.008100	20.167795
58.014127	2014.824852	20.172813
57.943233	2021.872220	20.177831
58.253432	2031.725060	20.182848
58.389069	2036.040538	20.187866
58.475771	2028.424473	20.192883
58.405959	2029.369165	20.197901
58.513878	2029.455276	20.202919
58.454660	2026.463480	20.207936
58.471988	2029.274495	20.212954
58.539154	2022.885317	20.217971
58.245355	2030.055032	20.222989
58.353013	2031.812091	20.228007
59.046687	2042.459337	20.233024
58.517594	2065.016036	20.238042
59.064501	2050.964940	20.243059
58.696923	2061.528464	20.248077
58.819068	2049.943824	20.253095
58.712433	2053.759251	20.258112
58.804362	2049.062461	20.263130
59.394830	2045.525280	20.268147
59.350137	2051.766730	20.273165
59.576503	2050.920215	20.278183
59.303076	2041.248367	20.283200
59.599564	2059.445427	20.288218
59.853012	2049.128448	20.293235
59.574026	2057.123695	20.298253
59.758363	2044.400781	20.303271
59.577654	2045.678411	20.308288
59.416606	2050.005615	20.313306
59.583971	2064.272784	20.318323
59.922657	2065.080547	20.323341
59.874853	2068.703555	20.328359
60.211619	2065.407202	20.333376
59.850679	2071.327391	20.338394
60.239698	2070.794109	20.343411
60.261312	2073.806003	20.348429
60.259460	2072.522853	20.353447
60.496278	2066.042573	20.358464
60.607832	2072.101857	20.363482
60.582049	2068.501350	20.368499
60.384425	2069.583746	20.373517
60.113422	2071.220825	20.378535
60.263349	2067.915250	20.383552
60.173221	2060.426876	20.388570
60.441092	2062.688526	20.393587
60.329174	2093.954367	20.398605
60.764708	2097.226872	20.403623
61.197594	2098.773391	20.408640
60.759033	2115.818173	20.413658
60.955736	2094.562222	20.418675
61.105641	2097.667448	20.423693
60.994640	2096.299610	20.428711
61.221174	2093.926252	20.433728
61.289740	2097.849692	20.438746
61.335626	2095.968462	20.443763
61.165025	2098.506662	20.448781
61.328738	2091.529801	20.453799
61.480632	2092.578736	20.458816
61.312294	2094.237796	20.463834
61.475318	2103.289832	20.468851
61.695136	2105.035809	20.473869
61.874250	2111.388654	20.478887
61.858519	2119.655707	20.483904
62.009333	2119.152810	20.488922
62.251852	2106.909202	20.493939
62.227500	2108.791673	20.498957
62.224813	2108.135448	20.503975
62.141741	2103.344779	20.508992
61.666088	2107.722122	20.514010
62.041675	2110.648247	20.519027
62.296770	2106.767753	20.524045
62.183758	2107.808188	20.529063
62.203344	2095.721189	20.534080
62.343972	2114.478387	20.539098
62.070603	2110.449955	20.544115
62.340160	2129.290550	20.549133
62.612533	2133.980671	20.554151
62.929077	2136.465776	20.559168
62.814834	2131.081423	20.564186
62.944818	2128.028357	20.569203
62.880110	2129.526163	20.574221
62.682496	2138.877310	20.579239
62.839660	2137.362308	20.584256
62.911366	2134.616930	20.589274
63.025427	2132.097224	20.594291
63.243140	2134.486091	20.599309
63.132833	2139.715575	20.604327
63.420531	2136.810414	20.609344
63.323252	2160.559176	20.614362
63.553984	2156.930743	20.619379
63.629748	2157.601725	20.624397
63.769069	2155.704624	20.629415
63.815897	2152.078296	20.634432
63.859156	2153.858630	20.639450
64.036067	2150.162337	20.644467
63.993536	2135.911116	20.649485
63.701060	2124.803351	20.654503
64.051077	2135.235509	20.659520
63.697153	2151.555272	20.664538
63.744393	2149.534437	20.669555
64.119465	2150.698396	20.674573
63.958661	2155.923254	20.679591
64.096108	2150.809829	20.684608
63.622123	2157.751161	20.689626
64.066898	2159.150438	20.694643
64.311560	2167.255894	20.699661
64.464932	2180.733730	20.704679
64.527659	2167.364294	20.709696
64.213185	2183.527947	20.714714
64.559912	2170.572523	20.719731
65.074758	2164.319405	20.724749
64.933940	2177.519955	20.729767
65.008582	2171.602329	20.734784
65.020446	2170.579113	20.739802
64.889479	2162.794686	20.744819
65.084165	2167.556737	20.749837
64.877659	2174.756160	20.754855
65.622760	2163.954930	20.759872
65.326474	2172.325160	20.764890
65.328599	2167.247915	20.769907
65.617588	2177.694143	20.774925
65.384354	2187.450443	20.779943
65.703859	2180.356406	20.784960
65.732384	2186.288926	20.789978
66.113391	2184.523463	20.794995
65.584354	2168.705073	20.800013
65.713686	2187.046500	20.805031
66.012417	2182.415037	20.810048
65.974216	2194.760395	20.815066
66.106465	2183.813766	20.820083
66.329950	2187.028092	20.825101
66.165555	2185.256080	20.830119
66.048618	2181.719855	20.835136
66.417960	2177.862949	20.840154
66.100571	2179.628196	20.845171
66.191286	2184.110214	20.850189
66.122986	2186.264941	20.855207
66.029127	2183.149711	20.860224
66.066308	2204.662031	20.865242
66.315207	2206.670537	20.870259
66.548394	2208.256039	20.875277
66.305905	2212.902688	20.880295
66.607478	2211.301167	20.885312
66.690699	2215.978930	20.890330
66.976788	2240.707288	20.895347
66.994473	2228.632705	20.900365
67.060159	2243.937778	20.905383
67.067281	2241.171972	20.910400
66.941498	2239.558528	20.915418
67.382692	2239.383152	20.920435
67.453357	2238.536422	20.925453
67.117157	2235.643204	20.930471
67.290057	2234.840179	20.935488
67.555400	2251.470518	20.940506
67.726972	2265.115105	20.945523
67.931531	2268.314076	20.950541
67.901978	2260.540762	20.955559
68.066809	2252.836058	20.960576
68.145452	2258.392971	20.965594
68.049039	2264.884417	20.970611
67.748829	2255.600743	20.975629
68.082003	2265.741672	20.980647
68.267123	2253.120824	20.985664
68.368684	2256.474647	20.990682
68.109546	2256.694373	20.995699
68.339205	2255.658319	21.000717
68.175888	2259.263882	21.005735
68.558377	2253.030676	21.010752
68.492593	2251.054921	21.015770
68.381565	2254.821122	21.020787
68.695144	2243.323543	21.025805
68.489061	2246.048750	21.030823
68.851192	2250.257099	21.035840
68.909226	2265.361484	21.040858
69.057897	2266.839721	21.045875
69.343607	2265.049870	21.050893
69.173530	2268.056925	21.055911
69.323496	2273.312259	21.060928
69.478754	2265.129587	21.065946
69.490443	2271.067290	21.070963
69.814892	2258.406044	21.075981
69.532692	2263.914434	21.080999
69.580250	2269.704459	21.086016
69.762930	2265.565435	21.091034
69.826837	2260.931884	21.096051
69.728040	2259.556105	21.101069
69.743575	2266.679434	21.106087
69.413588	2260.741365	21.111104
69.889420	2264.206061	21.116122
69.960317	2263.966008	21.121139
70.086588	2261.126137	21.126157
69.764193	2260.900808	21.131175
70.119447	2251.940907	21.136192
70.315760	2261.260368	21.141210
69.888676	2289.893253	21.146227
70.301340	2281.306521	21.151245
70.055411	2294.665131	21.156263
70.464624	2286.524261	21.161280
70.258363	2286.647827	21.166298
70.387936	2301.123842	21.171315
70.612837	2302.837897	21.176333
70.470945	2314.788690	21.181351
70.667976	2325.890035	21.186368
70.658734	2320.499648	21.191386
70.496624	2320.680868	21.196403
71.027801	2324.782110	21.201421
71.101133	2344.447616	21.206439
71.400803	2346.059922	21.211456
71.451629	2345.624757	21.216474
71.188616	2346.925488	21.221491
71.615174	2337.058023	21.226509
71.425863	2339.873781	21.231527
71.855177	2343.049334	21.236544
71.848447	2329.707795	21.241562
71.658747	2328.965984	21.246579
71.874063	2335.002284	21.251597
71.872945	2338.345566	21.256615
72.110167	2332.873027	21.261632
72.071508	2335.388237	21.266650
71.656164	2336.979160	21.271667
72.711569	2351.207435	21.276685
72.592185	2355.516407	21.281703
72.431969	2356.649323	21.286720
72.607836	2349.766402	21.291738
72.661969	2349.740156	21.296755
72.626055	2351.285187	21.301773
72.711392	2354.354697	21.306791
72.637058	2353.853638	21.311808
72.937462	2344.792918	21.316826
72.671711	2359.165932	21.321843
72.967850	2351.467392	21.326861
72.889802	2351.490986	21.331879
72.982998	2349.348338	21.336896
72.874707	2345.776783	21.341914
73.061611	2352.778860	21.346931
72.903472	2345.344524	21.351949
72.861938	2353.171861	21.356967
72.782231	2369.737405	21.361984
73.164840	2375.134577	21.367002
73.096606	2383.563227	21.372019
73.371902	2378.431628	21.377037
73.292837	2390.517752	21.382055
73.534469	2393.349965	21.387072
73.655531	2408.290109	21.392090
73.899112	2414.548543	21.397107
74.448472	2399.088396	21.402125
74.234678	2402.009009	21.407143
73.940353	2400.369515	21.412160
74.324476	2392.956401	21.417178
74.349337	2406.993138	21.422195
74.607762	2401.282801	21.427213
74.198258	2404.856322	21.432231
74.174168	2396.455628	21.437248
74.620840	2396.936068	21.442266
74.388231	2399.349930	21.447283
74.786270	2401.779064	21.452301
74.720750	2425.543839	21.457319
74.852651	2427.570172	21.462336
75.091969	2432.956442	21.467354
75.317677	2424.529334	21.472371
75.399227	2429.195233	21.477389
75.105504	2428.235590	21.482407
75.224413	2425.396908	21.487424
75.685889	2421.624693	21.492442
75.260672	2419.349357	21.497459
75.315048	2419.275824	21.502477
75.393829	2420.804234	21.507495
75.670440	2425.801631	21.512512
75.542101	2408.284682	21.517530
75.501295	2421.703930	21.522547
75.593771	2416.191151	21.527565
75.509330	2440.246497	21.532583
75.804513	2446.438523	21.537600
76.114483	2441.066899	21.542618
76.097447	2451.629340	21.547635
75.995020	2447.776856	21.552653
76.019738	2451.191478	21.557671
75.999035	2450.411049	21.562688
76.361406	2458.744426	21.567706
76.132855	2464.253058	21.572723
76.578982	2468.754662	21.577741
76.364549	2468.813043	21.582759
76.575053	2464.614238	21.587776
76.764549	2463.232835	21.592794
76.867850	2484.362529	21.597811
77.020129	2490.588077	21.602829
77.376872	2493.104383	21.607847
77.517820	2491.310914	21.612864
77.531296	2491.034694	21.617882
77.365739	2479.847782	21.622899
77.635456	2478.716494	21.627917
77.639463	2472.061985	21.632935
77.652735	2465.398465	21.637952
77.694619	2456.832476	21.642970
77.803472	2483.581218	21.647987
77.694338	2481.600406	21.653005
77.843229	2473.830119	21.658023
77.918529	2480.314484	21.663040
78.239907	2474.244073	21.668058
77.844644	2488.110275	21.673075
78.042391	2482.519017	21.678093
78.092344	2485.003043	21.683111
78.008147	2484.773704	21.688128
77.947710	2486.487778	21.693146
77.772962	2499.747371	21.698163
78.118369	2504.137308	21.703181
78.429011	2509.232647	21.708199
78.231631	2520.434477	21.713216
78.821830	2520.596653	21.718234
78.659646	2523.747340	21.723251
78.873348	2513.431911	21.728269
78.743381	2517.187531	21.733287
78.476198	2520.963509	21.738304
79.136673	2525.924549	21.743322
78.784305	2532.824254	21.748339
79.228037	2531.719665	21.753357
79.489668	2535.510851	21.758375
79.485798	2531.227044	21.763392
79.474478	2524.519142	21.768410
79.656176	2530.174449	21.773427
79.802035	2521.898707	21.778445
79.437786	2524.160752	21.783463
79.561493	2534.144404	21.788480
80.094945	2538.669368	21.793498
79.643805	2559.076745	21.798515
79.984181	2550.689642	21.803533
80.522956	2557.672924	21.808551
80.411703	2558.899328	21.813568
80.479244	2548.446256	21.818586
80.749899	2544.307554	21.823603
80.784757	2549.258007	21.828621
80.471765	2541.131459	21.833639
80.144548	2535.109357	21.838656
80.932426	2534.524590	21.843674
80.813641	2537.917320	21.848691
81.088118	2531.494003	21.853709
80.750263	2546.051971	21.858727
80.784317	2557.322207	21.863744
81.226583	2553.345650	21.868762
81.280951	2568.272186	21.873779
81.398846	2569.526796	21.878797
81.478390	2564.483456	21.883815
81.400740	2581.433947	21.888832
81.610971	2567.774375	21.893850
81.379614	2572.102733	21.898867
81.575641	2566.890491	21.903885
81.759393	2570.712298	21.908903
81.557388	2567.235741	21.913920
81.671145	2567.746504	21.918938
81.577501	2581.828219	21.923955
81.644980	2594.427277	21.928973
82.021803	2602.244135	21.933991
82.089022	2593.875463	21.939008
82.265362	2594.260898	21.944026
82.258140	2604.620232	21.949043
82.333654	2606.958304	21.954061
82.816124	2615.726632	21.959079
82.647541	2607.840723	21.964096
82.786429	2610.768732	21.969114
82.980997	2617.973216	21.974131
83.021314	2608.913672	21.979149
83.094685	2603.977254	21.984167
83.011359	2616.773751	21.989184
83.132094	2607.031561	21.994202
83.267937	2605.008597	21.999219
83.286115	2605.898595	22.004237
83.446977	2597.533708	22.009255
83.133400	2604.315204	22.014272
83.405449	2605.084029	22.019290
83.309441	2615.095056	22.024307
83.420027	2628.702421	22.029325
83.804420	2621.868324	22.034343
83.829480	2637.838426	22.039360
83.573748	2633.498254	22.044378
83.348854	2630.901117	22.049395
83.667208	2645.687162	22.054413
83.889470	2653.021731	22.059431
84.214144	2663.018651	22.064448
84.281717	2651.561898	22.069466
84.279781	2656.782667	22.074483
84.361818	2654.978067	22.079501
84.695798	2646.730563	22.084519
84.536751	2657.871810	22.089536
85.204973	2660.696044	22.094554
85.371680	2672.813352	22.099571
84.981113	2663.597939	22.104589
85.237586	2639.825677	22.109607
85.119092	2651.698834	22.114624
85.240605	2659.274904	22.119642
85.524188	2677.009443	22.124659
85.466124	2668.746519	22.129677
85.650048	2660.835684	22.134695
85.329409	2671.933219	22.139712
85.693035	2673.295193	22.144730
85.803152	2663.062175	22.149747
85.792973	2667.380712	22.154765
86.150737	2666.465557	22.159783
85.713304	2662.252318	22.164800
86.277200	2657.986288	22.169818
86.212741	2656.862284	22.174835
86.088285	2661.187929	22.179853
86.276341	2657.540068	22.184871
86.051540	2686.042936	22.189888
86.440943	2686.612796	22.194906
86.647810	2683.160253	22.199923
86.715710	2686.196100	22.204941
86.973147	2679.460169	22.209959
86.964381	2686.101855	22.214976
86.993137	2678.935647	22.219994
86.828601	2679.898030	22.225011
87.020936	2685.073650	22.230029
87.241982	2685.328843	22.235047
86.824930	2691.364467	22.240064
87.230290	2698.051772	22.245082
87.201844	2700.711816	22.250099
87.043677	2714.024754	22.255117
87.333742	2709.507967	22.260135
87.317595	2725.418047	22.265152
87.658632	2736.460014	22.270170
87.970192	2741.146589	22.275187
87.756856	2742.710010	22.280205
87.998106	2739.138762	22.285223
87.956959	2742.867131	22.290240
88.071138	2746.891065	22.295258
87.996852	2748.537377	22.300275
88.030858	2768.172920	22.305293
88.336248	2775.513076	22.310311
88.039268	2779.454690	22.315328
88.473648	2773.424120	22.320346
88.821566	2767.029101	22.325363
88.453517	2789.368040	22.330381
88.871720	2797.009629	22.335399
88.887749	2799.243004	22.340416
89.069204	2794.760318	22.345434
89.244797	2794.694275	22.350451
89.399443	2794.799429	22.355469
89.912069	2790.751317	22.360487
89.620759	2790.560597	22.365504
89.839431	2784.214531	22.370522
89.812781	2784.789892	22.375539
89.546522	2786.182932	22.380557
89.944124	2785.503319	22.385575
90.040992	2776.537078	22.390592
89.906883	2774.757620	22.395610
89.862082	2771.267588	22.400627
89.802337	2777.666162	22.405645
90.070456	2778.667160	22.410663
90.036241	2801.865081	22.415680
90.360556	2805.408930	22.420698
90.564625	2798.869200	22.425715
90.794263	2810.347410	22.430733
90.525538	2799.530525	22.435751
90.939574	2800.738484	22.440768
91.100254	2797.443968	22.445786
91.041377	2793.915706	22.450803
91.081787	2799.066909	22.455821
91.115686	2792.720329	22.460839
91.523709	2791.242869	22.465856
91.265787	2795.943036	22.470874
91.234688	2794.011866	22.475891
91.105006	2819.005669	22.480909
91.450527	2816.887326	22.485927
91.448431	2833.509810	22.490944
91.404763	2826.389386	22.495962
91.890352	2830.471542	22.500979
91.478901	2837.568971	22.505997
92.124133	2849.760349	22.511015
92.432940	2857.355116	22.516032
92.054723	2857.463451	22.521050
92.407434	2853.701663	22.526067
92.461847	2849.753026	22.531085
92.850732	2845.071796	22.536103
92.570020	2851.456194	22.541120
92.408571	2846.138862	22.546138
92.885602	2834.175171	22.551155
92.814340	2842.396680	22.556173
92.971692	2850.523645	22.561191
93.239101	2865.044693	22.566208
93.156200	2862.840180	22.571226
93.351887	2865.498578	22.576243
93.372168	2864.479435	22.581261
93.507169	2865.020159	22.586279
93.281783	2868.567628	22.591296
92.962778	2866.645926	22.596314
93.476883	2875.040239	22.601331
93.281443	2897.625577	22.606349
93.621739	2888.444544	22.611367
93.540316	2898.988026	22.616384
93.613923	2903.903827	22.621402
94.118512	2913.009242	22.626419
94.214791	2926.301887	22.631437
94.479528	2917.770013	22.636455
94.165112	2916.544844	22.641472
94.330405	2929.861109	22.646490
94.920912	2914.018416	22.651507
94.383144	2921.489975	22.656525
94.690288	2937.032546	22.661543
95.173731	2952.033696	22.666560
95.313798	2950.959672	22.671578
95.286051	2945.543784	22.676595
95.435668	2951.045490	22.681613
95.601517	2940.881810	22.686631
95.576741	2935.428029	22.691648
95.408112	2947.999137	22.696666
95.960702	2935.722048	22.701683
95.479786	2943.463754	22.706701
95.907356	2932.794110	22.711719
95.804322	2938.771929	22.716736
95.807269	2942.014660	22.721754
96.317317	2936.798733	22.726771
96.272402	2940.175775	22.731789
96.403123	2941.782652	22.736807
96.259166	2925.900515	22.741824
96.193691	2937.150888	22.746842
96.175546	2931.216838	22.751859
96.360169	2951.599784	22.756877
96.447545	2956.702315	22.761895
96.526528	2960.171456	22.766912
96.628732	2959.068264	22.771930
96.731739	2960.576180	22.776947
96.640329	2983.379477	22.781965
97.066388	2983.294407	22.786983
97.088668	2989.131803	22.792000
96.777269	2983.327790	22.797018
97.224506	2994.840982	22.802035
97.214787	3016.956335	22.807053
97.120495	3020.528200	22.812071
97.537517	3015.643032	22.817088
97.735796	3015.976023	22.822106
97.944524	3029.175723	22.827123
98.232890	3042.249640	22.832141
98.451317	3033.103269	22.837159
98.672613	3033.639948	22.842176
98.729098	3034.208640	22.847194
98.795731	3035.345387	22.852211
98.698384	3031.427343	22.857229
98.938548	3033.990604	22.862247
98.904763	3032.938272	22.867264
98.799590	3036.413903	22.872282
99.389796	3032.848204	22.877299
99.219057	3031.711058	22.882317
99.423211	3031.756044	22.887335
99.661869	3025.759359	22.892352
99.320539	3032.452318	22.897370
99.144960	3029.719771	22.902387
99.087843	3030.536820	22.907405
98.994031	3036.569848	22.912423
99.399789	3040.147909	22.917440
99.559198	3054.415732	22.922458
99.546299	3055.201048	22.927475
99.559352	3067.047228	22.932493
99.531298	3082.822231	22.937511
99.895813	3086.072456	22.942528
100.159559	3085.751244	22.947546
100.115421	3090.818895	22.952563
100.181358	3108.317890	22.957581
100.738132	3109.812901	22.962599
100.811071	3105.223279	22.967616
100.838739	3108.320599	22.972634
101.247565	3104.386454	22.977651
101.298742	3108.214989	22.982669
101.204548	3107.810114	22.987687
101.800285	3095.876970	22.992704
101.600992	3103.878060	22.997722
101.508942	3103.412588	23.002739
101.436372	3097.985563	23.007757
101.531412	3096.263413	23.012775
101.635569	3100.815918	23.017792
101.568321	3122.084568	23.022810
101.778057	3122.923587	23.027827
101.844596	3128.668266	23.032845
101.533535	3123.933535	23.037863
101.812034	3123.903609	23.042880
101.854098	3137.395192	23.047898
102.267117	3149.115365	23.052915
102.124647	3144.364920	23.057933
102.253208	3155.311251	23.062951
102.298683	3160.127844	23.067968
102.279762	3181.196822	23.072986
102.651388	3170.174040	23.078003
102.707799	3175.959394	23.083021
102.608666	3189.732693	23.088039
103.282396	3191.973777	23.093056
103.247413	3216.652901	23.098074
103.500754	3200.854326	23.103091
103.419525	3208.864665	23.108109
103.620577	3211.384426	23.113127
104.198624	3194.059510	23.118144
104.070691	3203.952565	23.123162
104.192716	3195.467006	23.128179
103.817334	3210.371601	23.133197
104.031743	3211.149608	23.138215
104.448578	3233.360803	23.143232
104.305905	3224.449715	23.148250
104.374958	3230.214884	23.153267
104.658303	3234.330240	23.158285
104.596068	3228.549454	23.163303
104.899102	3222.285317	23.168320
104.724878	3227.377701	23.173338
105.031842	3226.001589	23.178355
105.088612	3236.028274	23.183373
105.204251	3243.915869	23.188391
105.350750	3250.009595	23.193408
105.624103	3258.105755	23.198426
105.566579	3253.158518	23.203443
105.486000	3248.703337	23.208461
105.480215	3252.420066	23.213479
105.805163	3253.774717	23.218496
105.722662	3271.044902	23.223514
106.073131	3274.231738	23.228531
106.206373	3274.264448	23.233549
106.171318	3286.614873	23.238567
106.452853	3272.110905	23.243584
105.822068	3285.571878	23.248602
106.145043	3301.396474	23.253619
106.356979	3307.520731	23.258637
106.415575	3313.186076	23.263655
107.078407	3309.003111	23.268672
106.807587	3324.279518	23.273690
107.018180	3325.425526	23.278707
107.566032	3332.819908	23.283725
107.077844	3343.239676	23.288743
107.246983	3334.805697	23.293760
107.868973	3338.296842	23.298778
107.463002	3324.914241	23.303795
107.541877	3336.527262	23.308813
107.964510	3345.183854	23.313831
108.166585	3345.523313	23.318848
108.112882	3346.584326	23.323866
108.180273	3360.290436	23.328883
108.203787	3351.505321	23.333901
108.345811	3356.731233	23.338919
108.626050	3354.401164	23.343936
108.698977	3350.154423	23.348954
108.667187	3337.784778	23.353971
109.144504	3341.401856	23.358989
108.752115	3344.747529	23.364007
108.880965	3355.264379	23.369024
109.144038	3367.145777	23.374042
108.751727	3374.518261	23.379059
109.113034	3368.627925	23.384077
109.456725	3370.933524	23.389095
109.600560	3366.400992	23.394112
109.408542	3368.149153	23.399130
109.904592	3384.524375	23.404147
109.910246	3394.508832	23.409165
109.735720	3394.310184	23.414183
110.448532	3382.025908	23.419200
110.157474	3395.750841	23.424218
110.164756	3384.771301	23.429235
110.401628	3386.606345	23.434253
110.383349	3391.077621	23.439271
110.647857	3400.469951	23.444288
110.579847	3413.639015	23.449306
110.701646	3405.183304	23.454323
110.823725	3418.628021	23.459341
110.855267	3412.348123	23.464359
110.754155	3414.763204	23.469376
111.049757	3435.402849	23.474394
111.118952	3439.044209	23.479411
111.033739	3447.026192	23.484429
111.216641	3457.287676	23.489447
111.432495	3464.181908	23.494464
111.241572	3477.663141	23.499482
111.544546	3478.844659	23.504499
111.638337	3496.561550	23.509517
111.974886	3502.043133	23.514535
112.360318	3495.327399	23.519552
112.584528	3498.493056	23.524570
112.330550	3499.082455	23.529587
112.879385	3509.799196	23.534605
112.643510	3517.399812	23.539623
113.050267	3521.429057	23.544640
113.097609	3525.015386	23.549658
113.433520	3519.667058	23.554675
113.317513	3531.253822	23.559693
113.260043	3532.278853	23.564711
113.606963	3521.732414	23.569728
113.261150	3524.651072	23.574746
113.434365	3527.590110	23.579763
113.905834	3534.666488	23.584781
113.707880	3533.921651	23.589799
114.166657	3538.225786	23.594816
114.020995	3548.181449	23.599834
114.254057	3542.402844	23.604851
114.466565	3544.168704	23.609869
114.540419	3569.454062	23.614887
114.722314	3573.275638	23.619904
114.989279	3577.680053	23.624922
114.784493	3580.907303	23.629939
115.024021	3565.970989	23.634957
114.880587	3580.523713	23.639975
115.188812	3575.670955	23.644992
115.215880	3567.880133	23.650010
114.860329	3571.836759	23.655027
115.211966	3589.865833	23.660045
115.213003	3602.381813	23.665063
115.866678	3601.920041	23.670080
115.676419	3594.934181	23.675098
115.787568	3610.593350	23.680115
116.060895	3625.451965	23.685133
115.809074	3630.737269	23.690151
115.880450	3625.654778	23.695168
116.094281	3630.203455	23.700186
116.135896	3650.121954	23.705203
116.688774	3645.165275	23.710221
116.808663	3645.668761	23.715239
116.690693	3640.453420	23.720256
116.882018	3641.152192	23.725274
116.888738	3635.488989	23.730291
117.357446	3650.271967	23.735309
116.973153	3667.472854	23.740327
117.747606	3665.487350	23.745344
117.761567	3669.902179	23.750362
117.627662	3676.710300	23.755379
117.685737	3663.399416	23.760397
117.920579	3668.645897	23.765415
118.034879	3663.267273	23.770432
118.051103	3668.081385	23.775450
117.926931	3680.233856	23.780467
118.281110	3681.026548	23.785485
118.418703	3700.951271	23.790503
118.452259	3691.941439	23.795520
118.766325	3695.789987	23.800538
118.679650	3697.371511	23.805555
118.688188	3706.813886	23.810573
118.967788	3715.047064	23.815591
118.893193	3727.983593	23.820608
119.129395	3723.836506	23.825626
119.304197	3723.104758	23.830643
119.473394	3733.416731	23.835661
119.632741	3745.576256	23.840679
119.730506	3742.610900	23.845696
120.364556	3741.294781	23.850714
120.229206	3741.359757	23.855731
120.041312	3735.245997	23.860749
119.911044	3743.557681	23.865767
120.199279	3761.991598	23.870784
120.545871	3769.504563	23.875802
120.388342	3776.702910	23.880819
120.565777	3769.112714	23.885837
120.232798	3783.498950	23.890855
120.657111	3786.789825	23.895872
121.278282	3794.468394	23.900890
121.252713	3800.094694	23.905907
121.377064	3794.800988	23.910925
121.141510	3818.800391	23.915943
121.463317	3833.890581	23.920960
121.368356	3827.613348	23.925978
121.425518	3834.184362	23.930995
121.562331	3835.839937	23.936013
121.781231	3855.363546	23.941031
121.845318	3858.138800	23.946048
122.199277	3860.873937	23.951066
122.325949	3876.620972	23.956083
122.563181	3876.341151	23.961101
122.659835	3879.845372	23.966119
122.875638	3880.780687	23.971136
123.335288	3879.335536	23.976154
123.097940	3881.173159	23.981171
123.376545	3868.919445	23.986189
123.353521	3886.955373	23.991207
123.116471	3896.952769	23.996224
124.006285	3909.664809	24.001242
123.799641	3916.646122	24.006259
123.790425	3900.365829	24.011277
123.537383	3911.949573	24.016295
123.779870	3905.625102	24.021312
124.253460	3919.419985	24.026330
124.119274	3936.532113	24.031347
124.397847	3933.259187	24.036365
124.544023	3948.160424	24.041383
124.743113	3932.005082	24.046400
125.227187	3934.704515	24.051418
124.726271	3940.092195	24.056435
124.938236	3928.986247	24.061453
124.761648	3951.341602	24.066471
124.859151	3961.535655	24.071488
125.014521	3964.421423	24.076506
124.795913	3960.824054	24.081523
125.308557	3977.322762	24.086541
125.146948	3988.463802	24.091559
125.611010	3991.506373	24.096576
125.959419	4005.213773	24.101594
126.049789	4018.559909	24.106611
126.307151	4018.088142	24.111629
126.560520	4023.347820	24.116647
126.494401	4018.972321	24.121664
126.462304	4017.745994	24.126682
126.505585	4027.810464	24.131699
127.224687	4030.821843	24.136717
127.084164	4042.702063	24.141735
126.999794	4043.813876	24.146752
127.358776	4042.781895	24.151770
127.240080	4047.744071	24.156787
127.434196	4035.620375	24.161805
127.654457	4051.020939	24.166823
127.787888	4064.984490	24.171840
127.969785	4064.040890	24.176858
128.187415	4065.567343	24.181875
128.414416	4061.188979	24.186893
128.552797	4060.477815	24.191911
128.213649	4066.168727	24.196928
128.637332	4057.528020	24.201946
128.326848	4074.007179	24.206963
128.872445	4072.488324	24.211981
128.637456	4093.065086	24.216999
128.586857	4091.964671	24.222016
129.025050	4098.814498	24.227034
128.973321	4112.821347	24.232051
129.279000	4123.666187	24.237069
129.483727	4122.260464	24.242087
129.533244	4139.143942	24.247104
130.002711	4140.074291	24.252122
129.610877	4161.481173	24.257139
130.082432	4145.853428	24.262157
130.175925	4147.774518	24.267175
130.279182	4150.051528	24.272192
130.756327	4155.139534	24.277210
130.327700	4160.849232	24.282227
130.702599	4155.005969	24.287245
130.834338	4159.737711	24.292263
130.801183	4157.402711	24.297280
131.306685	4168.484621	24.302298
131.282411	4182.513763	24.307315
131.639580	4183.765118	24.312333
131.398980	4191.946461	24.317351
131.260486	4187.830969	24.322368
131.680455	4188.336375	24.327386
131.746070	4214.000575	24.332403
131.872677	4215.504313	24.337421
131.839459	4214.859353	24.342439
131.897913	4224.900175	24.347456
132.440039	4231.209145	24.352474
132.393772	4250.016000	24.357491
132.550239	4244.871182	24.362509
132.515432	4245.676330	24.367527
132.667911	4273.047001	24.372544
133.005131	4282.201409	24.377562
133.243049	4279.152109	24.382579
133.461137	4283.184439	24.387597
133.274657	4267.411145	24.392615
133.502345	4280.500086	24.397632
133.814063	4282.846557	24.402650
133.738682	4302.067811	24.407667
133.879241	4295.353692	24.412685
134.083558	4300.319172	24.417703
134.110111	4300.647156	24.422720
134.404198	4288.246828	24.427738
134.231965	4311.643881	24.432755
134.628826	4319.106263	24.437773
134.710284	4313.590311	24.442791
134.800828	4327.319424	24.447808
134.823683	4320.494050	24.452826
134.799969	4336.863792	24.457843
134.828904	4346.340977	24.462861
135.677340	4336.205143	24.467879
135.506912	4351.603744	24.472896
135.781942	4357.714426	24.477914
135.837433	4382.453647	24.482931
135.798546	4380.827560	24.487949
136.428642	4371.720937	24.492967
136.242229	4376.731441	24.497984
136.607343	4365.321830	24.503002
136.437624	4391.924650	24.508019
136.679164	4397.269105	24.513037
136.594347	4411.650267	24.518055
136.755229	4400.140561	24.523072
136.932132	4403.589086	24.528090
137.033458	4420.280793	24.533107
137.130547	4430.474432	24.538125
137.614894	4431.059757	24.543143
137.098277	4431.475308	24.548160
137.760800	4444.529409	24.553178
137.753468	4460.796549	24.558195
137.955910	4459.679416	24.563213
138.075798	4467.226314	24.568231
138.189719	4490.191148	24.573248
138.432599	4482.506295	24.578266
138.634406	4489.847481	24.583283
138.663156	4482.861190	24.588301
139.110999	4492.514035	24.593319
138.862772	4512.077604	24.598336
139.537122	4517.589858	24.603354
139.569155	4521.578236	24.608371
139.268684	4516.635775	24.613389
139.610304	4511.809099	24.618407
139.560000	4520.782091	24.623424
140.220558	4521.997422	24.628442
139.955700	4543.950046	24.633459
140.273103	4538.657994	24.638477
140.392396	4539.933010	24.643495
140.011897	4545.723869	24.648512
140.611334	4547.371446	24.653530
140.503239	4569.906927	24.658547
140.671024	4572.504085	24.663565
140.913194	4571.640258	24.668583
140.919254	4571.444771	24.673600
141.342624	4584.536221	24.678618
141.411747	4592.771238	24.683635
141.462469	4594.917615	24.688653
141.600103	4594.398714	24.693671
141.517393	4596.971194	24.698688
142.233289	4607.808309	24.703706
142.228254	4618.203264	24.708723
142.242685	4611.703630	24.713741
142.664606	4614.077585	24.718759
142.462768	4618.527622	24.723776
142.460590	4606.412359	24.728794
142.535999	4630.480831	24.733811
142.660533	4646.303417	24.738829
143.171429	4637.944862	24.743847
142.729155	4654.395256	24.748864
143.062893	4656.576691	24.753882
143.315397	4673.712231	24.758899
143.482394	4686.439047	24.763917
143.674795	4676.144629	24.768935
143.794795	4688.472062	24.773952
143.952456	4692.218382	24.778970
143.999944	4702.615724	24.783987
144.115476	4712.781291	24.789005
144.381484	4703.717431	24.794023
144.278555	4714.435016	24.799040
144.508014	4720.877857	24.804058
144.900484	4732.318319	24.809075
144.671485	4742.830766	24.814093
144.923257	4751.190776	24.819111
145.277406	4760.091431	24.824128
145.558258	4761.711446	24.829146
145.668580	4765.100982	24.834163
145.845395	4785.921556	24.839181
146.222115	4772.428214	24.844199
146.265518	4786.782190	24.849216
146.271749	4777.236782	24.854234
146.259450	4774.235901	24.859251
146.484280	4783.708482	24.864269
146.582661	4792.432559	24.869287
146.748457	4806.665483	24.874304
146.857839	4805.578697	24.879322
146.806647	4818.445699	24.884339
146.819810	4823.914741	24.889357
147.392823	4834.057415	24.894375
147.050481	4837.351795	24.899392
147.384739	4847.052018	24.904410
147.780920	4868.829499	24.909427
147.830186	4862.977671	24.914445
148.089061	4887.216990	24.919463
147.898994	4902.210634	24.924480
148.123217	4891.714705	24.929498
148.160877	4902.172085	24.934515
148.767045	4915.673010	24.939533
149.230220	4916.970670	24.944551
148.929809	4922.118354	24.949568
149.144677	4918.461598	24.954586
149.283668	4932.801457	24.959603
149.544931	4943.378571	24.964621
149.978533	4949.295481	24.969639
149.768619	4948.583661	24.974656
150.214859	4943.166974	24.979674
149.900451	4948.308321	24.984691
149.750881	4972.273588	24.989709
150.273682	4975.576767	24.994727
150.297192	4985.783736	24.999744
150.370481	4998.716122	25.004762
150.674324	5010.970055	25.009779
150.389181	5014.990592	25.014797
150.951997	5020.983796	25.019815
151.073592	5030.902844	25.024832
151.276923	5031.811944	25.029850
151.464079	5040.163904	25.034867
151.553687	5059.153998	25.039885
151.763436	5057.358303	25.044903
151.718838	5076.818766	25.049920
152.119100	5087.165833	25.054938
152.506290	5097.383547	25.059955
152.261681	5090.383175	25.064973
152.909751	5090.023900	25.069991
152.566745	5086.493331	25.075008
152.674116	5088.936762	25.080026
153.101355	5113.597474	25.085043
152.787098	5123.765155	25.090061
153.136888	5117.924910	25.095079
153.050551	5131.724962	25.100096
153.330980	5139.110929	25.105114
153.651326	5147.260541	25.110131
153.706508	5151.108996	25.115149
154.105459	5171.582999	25.120167
154.062711	5172.131970	25.125184
154.165603	5179.928537	25.130202
154.587592	5182.725499	25.135219
154.735930	5207.313607	25.140237
155.066736	5203.287119	25.145255
155.330262	5208.855034	25.150272
155.489728	5207.811910	25.155290
155.303702	5200.721456	25.160307
155.340190	5207.853287	25.165325
156.060056	5224.091396	25.170343
155.691812	5233.271009	25.175360
155.861947	5240.625666	25.180378
156.244963	5231.661846	25.185395
156.055284	5242.225608	25.190413
156.572388	5250.203297	25.195431
156.569001	5261.449780	25.200448
156.303918	5259.623199	25.205466
156.719053	5272.811886	25.210483
157.147443	5287.930332	25.215501
157.141647	5285.921419	25.220519
157.170646	5286.217516	25.225536
157.498744	5303.687765	25.230554
157.779795	5310.460970	25.235571
157.727497	5315.748849	25.240589
157.523625	5331.227976	25.245607
157.458625	5350.018767	25.250624
157.756414	5352.006994	25.255642
158.157715	5367.819139	25.260659
158.298032	5377.769960	25.265677
158.811229	5388.169413	25.270695
158.963588	5404.756841	25.275712
159.423858	5407.467174	25.280730
159.605222	5404.831843	25.285747
159.225368	5403.837826	25.290765
159.672420	5421.472809	25.295783
159.788556	5436.643092	25.300800
160.106221	5441.219215	25.305818
160.018119	5438.390638	25.310835
159.945256	5445.966766	25.315853
160.426659	5449.358812	25.320871
160.308377	5464.664805	25.325888
160.435278	5467.671342	25.330906
160.644409	5473.846140	25.335923
160.680178	5500.412084	25.340941
161.156005	5497.423190	25.345959
160.907772	5512.641268	25.350976
161.482369	5525.561189	25.355994
161.733013	5512.542533	25.361011
161.336981	5535.735083	25.366029
162.275471	5548.697955	25.371047
162.255734	5551.701218	25.376064
162.053764	5552.009567	25.381082
162.659999	5555.758229	25.386099
162.880713	5578.680980	25.391117
163.118411	5573.636485	25.396135
162.966985	5574.399574	25.401152
163.175455	5577.912443	25.406170
163.328354	5573.749919	25.411187
163.614157	5596.784787	25.416205
163.736985	5601.182923	25.421223
163.806177	5591.941638	25.426240
163.416655	5612.440424	25.431258
164.042687	5602.632024	25.436275
164.362623	5623.397720	25.441293
164.308792	5621.116332	25.446311
164.292460	5632.518016	25.451328
164.712779	5629.907672	25.456346
164.725175	5641.804733	25.461363
164.683133	5648.298418	25.466381
164.826534	5654.064377	25.471399
165.242576	5670.856527	25.476416
164.953730	5694.326916	25.481434
165.378936	5699.149158	25.486451
165.754139	5714.179156	25.491469
165.860550	5716.655137	25.496487
166.068995	5720.689436	25.501504
166.040890	5737.648124	25.506522
166.392687	5750.979229	25.511539
166.334271	5755.483812	25.516557
166.930838	5768.960285	25.521575
167.004592	5770.835223	25.526592
167.239350	5764.830273	25.531610
167.841532	5764.382499	25.536627
167.503937	5780.838783	25.541645
167.960586	5788.593625	25.546663
168.069061	5791.135435	25.551680
168.069233	5797.309512	25.556698
168.187341	5796.581151	25.561715
168.499713	5807.445740	25.566733
168.596249	5819.305377	25.571751
168.784007	5827.573382	25.576768
168.758339	5833.818697	25.581786
168.996123	5843.172420	25.586803
169.061539	5858.797294	25.591821
169.217702	5866.925630	25.596839
169.724820	5873.347395	25.601856
169.942385	5890.686949	25.606874
170.001597	5881.099810	25.611891
169.902619	5888.201605	25.616909
170.329636	5904.974861	25.621927
170.428921	5911.553159	25.626944
170.402272	5918.168850	25.631962
170.819379	5902.585408	25.636979
170.997201	5925.272392	25.641997
171.219881	5926.730461	25.647015
171.083609	5923.344264	25.652032
171.666842	5939.185149	25.657050
171.675412	5951.776966	25.662067
172.019098	5964.655141	25.667085
171.981531	5960.855635	25.672103
172.075983	5958.967874	25.677120
172.416599	5979.688872	25.682138
172.622803	5978.199258	25.687156
172.599007	5988.787250	25.692173
172.552834	5981.597680	25.697191
172.917489	5998.756266	25.702208
172.786982	6017.098724	25.707226
173.242815	6013.989391	25.712244
173.465566	6031.295161	25.717261
173.265669	6038.331817	25.722279
173.770643	6047.222413	25.727296
173.929460	6061.545052	25.732314
174.368412	6066.790449	25.737332
174.151418	6076.121934	25.742349
174.220007	6077.531491	25.747367
174.943755	6099.977911	25.752384
174.965023	6105.930443	25.757402
175.511970	6105.310654	25.762420
175.418428	6104.012423	25.767437
175.256929	6104.546430	25.772455
175.667551	6119.543386	25.777472
175.950494	6130.675349	25.782490
176.001580	6130.052585	25.787508
176.315680	6126.039659	25.792525
175.892201	6122.176407	25.797543
176.628332	6136.241289	25.802560
176.609249	6152.287645	25.807578
176.782880	6157.409231	25.812596
176.830220	6162.782502	25.817613
177.197231	6172.558461	25.822631
176.948740	6184.941767	25.827648
177.353078	6192.237619	25.832666
177.645316	6195.671386	25.837684
177.820528	6208.128702	25.842701
177.790891	6216.718810	25.847719
178.348016	6217.120463	25.852736
178.148714	6235.848688	25.857754
178.428040	6241.460039	25.862772
178.462192	6246.716589	25.867789
178.818297	6260.738953	25.872807
179.505261	6271.315011	25.877824
179.197200	6273.454852	25.882842
179.348617	6276.187328	25.887860
179.380173	6296.064368	25.892877
179.328622	6304.836944	25.897895
179.857229	6311.288414	25.902912
180.076446	6325.828132	25.907930
180.421251	6326.987987	25.912948
180.358614	6344.422473	25.917965
180.376365	6366.393847	25.922983
180.692697	6363.000364	25.928000
180.971669	6381.915804	25.933018
181.431507	6383.460678	25.938036
181.645564	6382.211532	25.943053
181.636830	6390.076010	25.948071
182.039202	6403.878180	25.953088
182.117505	6413.226350	25.958106
182.051110	6421.198844	25.963124
182.368334	6425.869846	25.968141
182.174586	6445.426783	25.973159
182.979414	6439.035779	25.978176
182.587017	6452.658446	25.983194
182.831142	6457.699148	25.988212
183.023038	6471.206986	25.993229
183.177945	6487.001974	25.998247
183.712417	6485.862031	26.003264
183.182868	6504.536549	26.008282
184.249166	6515.786422	26.013300
184.428009	6522.433720	26.018317
184.423168	6524.079952	26.023335
184.645386	6532.168553	26.028352
184.696088	6548.722027	26.033370
185.304366	6547.587189	26.038388
185.317084	6545.122943	26.043405
185.309090	6560.479474	26.048423
185.387280	6577.977543	26.053440
185.912015	6585.220565	26.058458
185.885702	6583.507890	26.063476
185.982658	6597.140249	26.068493
186.026524	6614.320316	26.073511
186.457351	6609.911450	26.078528
186.142053	6623.795601	26.083546
186.727149	6628.280541	26.088564
186.686498	6636.806538	26.093581
187.201289	6641.415754	26.098599
187.638332	6648.330695	26.103616
187.273722	6666.255821	26.108634
187.366557	6670.660010	26.113652
187.636613	6671.836992	26.118669
187.663842	6694.285357	26.123687
188.221984	6693.357299	26.128704
188.246918	6705.244419	26.133722
188.443263	6715.531801	26.138740
188.849009	6716.430336	26.143757
188.932146	6730.264374	26.148775
189.319999	6743.280014	26.153792
189.367271	6742.539709	26.158810
189.569655	6752.453554	26.163828
189.795234	6752.108277	26.168845
189.898301	6779.297714	26.173863
190.139590	6772.858881	26.178880
190.487330	6783.960887	26.183898
190.306575	6781.107237	26.188916
190.728204	6788.735259	26.193933
190.853009	6804.685202	26.198951
191.134095	6806.707102	26.203968
191.418463	6820.028221	26.208986
191.762503	6830.838651	26.214004
191.709504	6829.993642	26.219021
191.590535	6843.597370	26.224039
192.051397	6849.535696	26.229056
191.940531	6856.764342	26.234074
192.182326	6865.515446	26.239092
192.792360	6881.543459	26.244109
192.834989	6891.987943	26.249127
192.865931	6887.915369	26.254144
193.056478	6913.376599	26.259162
193.380828	6914.302799	26.264180
193.721987	6928.686619	26.269197
193.345821	6949.904054	26.274215
193.906606	6946.914224	26.279232
193.917275	6972.281663	26.284250
193.893480	6986.532973	26.289268
194.370944	6999.552894	26.294285
194.267040	7017.447858	26.299303
194.733265	7017.826778	26.304320
194.962525	7042.705233	26.309338
195.249100	7046.949063	26.314356
194.934520	7066.102211	26.319373
195.100112	7077.530742	26.324391
195.790926	7089.235450	26.329408
195.918634	7107.014981	26.334426
196.127230	7115.984392	26.339444
196.596996	7122.809844	26.344461
196.672673	7132.000550	26.349479
197.196387	7129.518573	26.354496
197.285705	7143.566983	26.359514
197.365718	7152.250507	26.364532
198.130104	7156.353829	26.369549
198.051577	7152.546640	26.374567
198.132981	7154.975789	26.379584
198.500631	7158.750951	26.384602
198.585196	7176.332905	26.389620
199.195872	7178.182929	26.394637
199.135954	7177.767543	26.399655
199.637025	7181.686036	26.404672
199.396841	7184.305482	26.409690
199.313773	7185.462982	26.414708
199.912502	7192.656229	26.419725
199.387333	7226.952893	26.424743
199.750412	7208.782505	26.429760
200.035845	7215.568410	26.434778
200.206794	7232.606806	26.439796
200.588654	7235.599831	26.444813
200.266453	7248.416786	26.449831
200.570879	7249.558192	26.454848
200.523665	7278.232934	26.459866
200.707558	7289.063888	26.464884
201.444807	7292.827521	26.469901
201.223847	7294.713621	26.474919
201.748361	7320.396694	26.479936
201.895409	7328.023960	26.484954
201.921804	7331.958844	26.489972
202.102420	7352.542714	26.494989
202.379072	7368.331817	26.500007
202.421052	7366.521105	26.505024
202.629833	7392.452697	26.510042
202.995798	7400.391916	26.515060
203.099586	7425.386264	26.520077
203.212698	7441.997291	26.525095
203.489684	7441.965657	26.530112
203.689589	7455.024813	26.535130
203.875295	7471.249700	26.540148
204.450579	7484.794185	26.545165
204.187043	7500.449139	26.550183
204.674384	7513.547406	26.555200
205.408847	7522.517428	26.560218
205.587258	7526.664290	26.565236
205.888375	7541.130914	26.570253
206.170910	7539.400090	26.575271
206.351696	7539.790833	26.580288
206.547258	7534.066615	26.585306
206.297917	7551.662512	26.590324
206.779483	7557.885189	26.595341
206.727784	7573.730428	26.600359
206.804925	7576.880302	26.605376
207.168763	7588.534747	26.610394
207.043361	7599.424992	26.615412
207.507656	7609.642603	26.620429
207.641148	7627.127947	26.625447
207.580087	7639.927191	26.630464
208.187383	7657.638974	26.635482
208.372885	7663.969781	26.640500
208.711443	7674.046770	26.645517
208.817245	7692.007815	26.650535
208.968405	7692.617721	26.655552
209.136955	7696.554368	26.660570
209.234527	7723.795167	26.665588
209.906601	7715.641492	26.670605
209.835786	7739.230041	26.675623
209.986782	7745.833625	26.680640
210.341384	7745.486664	26.685658
210.406478	7765.457665	26.690676
210.840030	7760.045287	26.695693
210.965706	7777.412358	26.700711
211.277674	7783.430826	26.705728
211.666864	7800.883485	26.710746
211.643811	7804.754989	26.715764
211.855008	7808.377399	26.720781
212.076059	7820.842573	26.725799
211.886870	7828.656501	26.730816
212.480988	7840.193453	26.735834
212.226754	7853.383255	26.740852
212.640488	7861.412474	26.745869
212.601178	7882.576170	26.750887
212.965320	7892.672695	26.755904
213.157349	7920.076216	26.760922
213.512209	7925.410992	26.765940
213.864014	7938.408377	26.770957
213.721378	7954.661329	26.775975
214.145218	7955.043356	26.780992
214.729350	7958.906546	26.786010
214.705373	7985.717341	26.791028
214.634949	7981.746342	26.796045
214.872063	7987.748922	26.801063
215.314746	8004.100384	26.806080
215.415731	8006.550054	26.811098
215.577747	8026.142199	26.816116
216.190563	8032.184217	26.821133
215.984121	8038.529643	26.826151
216.504206	8053.604841	26.831168
216.964451	8063.138100	26.836186
216.920286	8070.436600	26.841204
216.956934	8070.807105	26.846221
217.318328	8084.922375	26.851239
217.604361	8100.896555	26.856256
218.099246	8103.103008	26.861274
217.304456	8120.782735	26.866292
218.021188	8131.173944	26.871309
218.196683	8143.430289	26.876327
218.047123	8172.722252	26.881344
218.384193	8171.362807	26.886362
218.439491	8192.619171	26.891380
219.174843	8212.620780	26.896397
219.252559	8229.908058	26.901415
219.385434	8229.517446	26.906432
219.815356	8250.702419	26.911450
219.825108	8254.489829	26.916468
220.254683	8275.563823	26.921485
220.224973	8281.701273	26.926503
220.482846	8303.333083	26.931520
220.842211	8313.833198	26.936538
220.951443	8324.377091	26.941556
221.293050	8340.882697	26.946573
221.660189	8357.956779	26.951591
221.933108	8365.570008	26.956608
222.260229	8366.851898	26.961626
222.649787	8402.136359	26.966644
222.908236	8397.690951	26.971661
222.885064	8402.856873	26.976679
222.973101	8411.211269	26.981696
223.661789	8417.699341	26.986714
223.652375	8433.613268	26.991732
223.787878	8435.148238	26.996749
223.677200	8453.231051	27.001767
223.855662	8468.181227	27.006784
224.393682	8485.318535	27.011802
224.559097	8501.529713	27.016820
224.449904	8500.446566	27.021837
224.811109	8528.915726	27.026855
224.835006	8537.758967	27.031872
225.296514	8546.691259	27.036890
225.564438	8562.679928	27.041908
225.685644	8581.892728	27.046925
226.160878	8588.220844	27.051943
226.379987	8609.881544	27.056960
226.758836	8615.613546	27.061978
226.786068	8624.030898	27.066996
227.273344	8628.553881	27.072013
227.703368	8636.691083	27.077031
227.543036	8651.977165	27.082048
228.091490	8655.079955	27.087066
228.101633	8669.603650	27.092084
228.468750	8674.448246	27.097101
228.814585	8686.168711	27.102119
228.767039	8709.116758	27.107136
229.077693	8708.880252	27.112154
228.966922	8710.024329	27.117172
229.159109	8714.878200	27.122189
229.369734	8730.731577	27.127207
229.383524	8741.645245	27.132224
229.892546	8746.581385	27.137242
230.024536	8765.255371	27.142260
230.219530	8778.465311	27.147277
230.238830	8793.636714	27.152295
230.379056	8803.023304	27.157312
230.603731	8826.632288	27.162330
230.986180	8843.997402	27.167348
231.405625	8854.136588	27.172365
231.893402	8862.709430	27.177383
231.682749	8889.287165	27.182400
232.013748	8892.540225	27.187418
232.016240	8909.085226	27.192436
232.523154	8917.705347	27.197453
233.005754	8933.168863	27.202471
233.316249	8951.055688	27.207488
233.412559	8954.543764	27.212506
233.336953	8977.080900	27.217524
233.794781	8979.178601	27.222541
234.257465	8995.622304	27.227559
234.018771	9014.897563	27.232576
234.829339	9025.561364	27.237594
234.922421	9042.875337	27.242612
235.019773	9046.062333	27.247629
235.299560	9064.686206	27.252647
235.535228	9066.064435	27.257664
235.631129	9087.725695	27.262682
235.737233	9102.226807	27.267700
236.246156	9110.053414	27.272717
236.564947	9131.977191	27.277735
236.606988	9138.385115	27.282752
237.090596	9148.509929	27.287770
237.349116	9157.555733	27.292788
237.401570	9180.579283	27.297805
237.921568	9186.315700	27.302823
237.754659	9195.435100	27.307840
238.316878	9201.668710	27.312858
238.397161	9215.880359	27.317876
238.488209	9236.279816	27.322893
238.891854	9253.155019	27.327911
239.107929	9260.769422	27.332928
239.781991	9269.893030	27.337946
239.916216	9290.301163	27.342964
239.724227	9293.214690	27.347981
240.090422	9312.260191	27.352999
240.162740	9324.658992	27.358016
240.654247	9337.033315	27.363034
240.712387	9346.815887	27.368052
240.632702	9373.615380	27.373069
241.078358	9378.228974	27.378087
241.228578	9399.456259	27.383104
241.550501	9409.629275	27.388122
241.644199	9436.868906	27.393140
241.850667	9450.427280	27.398157
242.501567	9474.236876	27.403175
242.957411	9486.080734	27.408192
243.223577	9493.129987	27.413210
243.080441	9509.946292	27.418228
243.383351	9513.185224	27.423245
243.565122	9530.655993	27.428263
243.931345	9544.566931	27.433280
244.325955	9559.193226	27.438298
244.521967	9570.887148	27.443316
244.688207	9579.816904	27.448333
245.483053	9587.412073	27.453351
245.083297	9599.039198	27.458368
245.710667	9597.080127	27.463386
246.091033	9616.857872	27.468404
245.726959	9630.432851	27.473421
246.065553	9629.721395	27.478439
245.888492	9636.336739	27.483456
246.438782	9648.559770	27.488474
246.902841	9675.580940	27.493492
246.766993	9690.924616	27.498509
246.976957	9696.484077	27.503527
246.928600	9719.697617	27.508544
247.645339	9733.308054	27.513562
247.785340	9748.325665	27.518580
247.640021	9772.114671	27.523597
248.118174	9776.031310	27.528615
248.313967	9799.395198	27.533632
248.732885	9812.634313	27.538650
248.866845	9827.551372	27.543668
249.282523	9854.001812	27.548685
249.599612	9869.128089	27.553703
249.851644	9888.352311	27.558720
250.278801	9896.296044	27.563738
250.625812	9918.753514	27.568756
250.919273	9940.000344	27.573773
251.141805	9938.495853	27.578791
251.634931	9959.158977	27.583808
251.815276	9960.931684	27.588826
251.864941	9968.243088	27.593844
252.049682	9990.165807	27.598861
252.456992	9991.324266	27.603879
252.411974	10023.521157	27.608896
252.871005	10025.472268	27.613914
253.191467	10046.830579	27.618932
253.371032	10056.968485	27.623949
253.933018	10065.233474	27.628967
253.809364	10078.531109	27.633984
254.405124	10080.628188	27.639002
254.877619	10105.436487	27.644020
254.766999	10113.827019	27.649037
255.020330	10112.264629	27.654055
255.234709	10139.078170	27.659072
255.456798	10147.668901	27.664090
255.564570	10158.705057	27.669108
255.536052	10179.626558	27.674125
256.141711	10191.471351	27.679143
255.976607	10212.351691	27.684160
256.257625	10226.932798	27.689178
256.616082	10243.078331	27.694196
257.005579	10263.264244	27.699213
257.433978	10277.174981	27.704231
257.256749	10300.305908	27.709248
257.610962	10322.724934	27.714266
257.883665	10331.876200	27.719284
258.425199	10363.012370	27.724301
258.920704	10364.944093	27.729319
259.111932	10385.988631	27.734336
259.148781	10386.867311	27.739354
259.457830	10408.140542	27.744372
259.995271	10435.272958	27.749389
260.425617	10432.519966	27.754407
260.297643	10451.398876	27.759424
260.453185	10458.527531	27.764442
260.967526	10473.105692	27.769460
260.938147	10487.988949	27.774477
261.888347	10501.309289	27.779495
262.016452	10517.294693	27.784512
261.999617	10515.086049	27.789530
262.484649	10523.168630	27.794548
262.610634	10543.003805	27.799565
262.932912	10550.308953	27.804583
262.783008	10552.777697	27.809600
263.190125	10558.737350	27.814618
263.333060	10572.204769	27.819636
263.446154	10578.217826	27.824653
263.777678	10599.604979	27.829671
263.673483	10619.318417	27.834688
264.220596	10632.614988	27.839706
264.419074	10649.547684	27.844724
264.445823	10678.818178	27.849741
265.068832	10686.291054	27.854759
265.088638	10699.747447	27.859776
265.028195	10715.252942	27.864794
265.703522	10732.357329	27.869812
265.387972	10766.350302	27.874829
265.839044	10779.937066	27.879847
266.379066	10809.096047	27.884864
266.834555	10821.101676	27.889882
266.870479	10848.919728	27.894900
266.948890	10864.553650	27.899917
267.565294	10883.804625	27.904935
267.894246	10908.783678	27.909952
268.191985	10924.715406	27.914970
268.717435	10949.471334	27.919988
268.842392	10970.234519	27.925005
269.374418	10972.580993	27.930023
269.964719	10995.485808	27.935040
269.746642	10994.940502	27.940058
270.337179	11014.296762	27.945076
270.212882	11034.615963	27.950093
270.894642	11047.113753	27.955111
271.028164	11054.103713	27.960128
271.127186	11080.808705	27.965146
271.602127	11095.122927	27.970164
271.503599	11102.572041	27.975181
272.214835	11119.735503	27.980199
272.119792	11121.585440	27.985216
272.310896	11148.268998	27.990234
272.854069	11173.324879	27.995252
272.939330	11190.237489	28.000269
273.396601	11194.941086	28.005287
273.717472	11209.198973	28.010304
274.082552	11218.241696	28.015322
274.273684	11235.948342	28.020340
274.531451	11248.458169	28.025357
274.758279	11260.761976	28.030375
274.665391	11278.178469	28.035392
275.036865	11295.092661	28.040410
275.701292	11296.534845	28.045428
275.729590	11331.921786	28.050445
276.011436	11344.024306	28.055463
276.467254	11367.542822	28.060480
276.203625	11380.618089	28.065498
277.317395	11392.679063	28.070516
277.038949	11420.222374	28.075533
277.579291	11416.552823	28.080551
277.936002	11440.045304	28.085568
277.939303	11459.997247	28.090586
278.335890	11471.275649	28.095604
278.392482	11496.515000	28.100621
278.821835	11503.638978	28.105639
279.334638	11526.541618	28.110656
278.993938	11528.373959	28.115674
279.866104	11549.953372	28.120692
279.612034	11572.957802	28.125709
280.170968	11584.387476	28.130727
280.472586	11609.320136	28.135744
280.381158	11628.511102	28.140762
280.972732	11632.467734	28.145780
280.771905	11652.530916	28.150797
281.134480	11665.873071	28.155815
281.832374	11686.874834	28.160832
282.257553	11717.415956	28.165850
282.684078	11707.291796	28.170868
282.539654	11723.297503	28.175885
283.142806	11732.550086	28.180903
283.350081	11748.639424	28.185920
283.245499	11769.561390	28.190938
283.892101	11776.033390	28.195956
284.094581	11812.478279	28.200973
284.381808	11816.450666	28.205991
284.273822	11837.261400	28.211008
284.552923	11853.865276	28.216026
284.974892	11860.388674	28.221044
285.294895	11894.831921	28.226061
285.671806	11902.268890	28.231079
286.111541	11938.066524	28.236096
286.360485	11954.237416	28.241114
286.944415	11966.616597	28.246132
286.791670	11990.596039	28.251149
286.936928	12009.195163	28.256167
287.431992	12023.897685	28.261184
287.954299	12048.083794	28.266202
287.999451	12061.452028	28.271220
288.172502	12078.965609	28.276237
288.533919	12101.908306	28.281255
289.075975	12109.106872	28.286272
289.292806	12135.790951	28.291290
289.716899	12143.905712	28.296308
289.658479	12166.230926	28.301325
290.024227	12192.991304	28.306343
290.373640	12206.514155	28.311360
290.775496	12228.370882	28.316378
290.940173	12240.061685	28.321396
291.452858	12258.252014	28.326413
291.617024	12276.622968	28.331431
292.098706	12290.870951	28.336448
292.172721	12310.153527	28.341466
292.647815	12319.221207	28.346484
292.302982	12337.172206	28.351501
292.923987	12360.292921	28.356519
293.052509	12387.338720	28.361536
293.136999	12406.712652	28.366554
293.778069	12425.777011	28.371572
293.610103	12450.301749	28.376589
294.036528	12471.819076	28.381607
294.395532	12499.556541	28.386624
294.487475	12524.879888	28.391642
295.279822	12551.313377	28.396660
295.741955	12579.713113	28.401677
295.843244	12595.028166	28.406695
296.123226	12618.148964	28.411712
296.410530	12634.328368	28.416730
296.925281	12665.697975	28.421748
297.170334	12683.320059	28.426765
297.482095	12705.545341	28.431783
298.004967	12732.597356	28.436800
298.234982	12742.517428	28.441818
298.397920	12739.135411	28.446836
298.879713	12761.227041	28.451853
299.079815	12781.831973	28.456871
299.293102	12788.684983	28.461888
299.278801	12809.768268	28.466906
300.077754	12824.153315	28.471924
300.246409	12853.136339	28.476941
300.429372	12853.258959	28.481959
300.934002	12862.150283	28.486976
301.108004	12892.930606	28.491994
301.431013	12891.101128	28.497012
302.156629	12913.174670	28.502029
301.876030	12928.275885	28.507047
302.357166	12945.313909	28.512064
302.520937	12954.242792	28.517082
302.909440	12979.617042	28.522100
302.660862	12990.418627	28.527117
303.383338	13013.586517	28.532135
303.405803	13023.982374	28.537152
303.537107	13058.640554	28.542170
304.067384	13072.586483	28.547188
304.172862	13094.334264	28.552205
304.770904	13121.985948	28.557223
305.017960	13133.399002	28.562240
305.056032	13159.737700	28.567258
305.630418	13177.100936	28.572276
305.947035	13209.555541	28.577293
306.445183	13223.024679	28.582311
307.180590	13241.951462	28.587328
307.002568	13258.706507	28.592346
307.137407	13281.946829	28.597364
307.733864	13298.765991	28.602381
307.967987	13324.514618	28.607399
308.518226	13333.300943	28.612416
308.946396	13356.546403	28.617434
309.109944	13379.553599	28.622452
309.198039	13391.245298	28.627469
309.647614	13416.863852	28.632487
310.020503	13427.127894	28.637504
309.933329	13454.698140	28.642522
310.486313	13470.829674	28.647540
310.798500	13492.290039	28.652557
311.119589	13512.716697	28.657575
311.593051	13523.701710	28.662592
311.430096	13560.245670	28.667610
311.924126	13570.242323	28.672628
312.354936	13601.156411	28.677645
312.457523	13613.562943	28.682663
312.889951	13639.632265	28.687680
312.834685	13666.428504	28.692698
313.551825	13696.313539	28.697716
313.727135	13715.237444	28.702733
314.201441	13727.989144	28.707751
314.508394	13758.189616	28.712768
314.591300	13784.134204	28.717786
314.757839	13794.955865	28.722804
315.131407	13827.039792	28.727821
315.632131	13852.295963	28.732839
315.873259	13877.984415	28.737856
316.142091	13909.272618	28.742874
316.525365	13928.093003	28.747892
317.005632	13950.664034	28.752909
317.186874	13973.856683	28.757927
317.459703	13998.135845	28.762944
317.571051	14017.548221	28.767962
318.306149	14048.195299	28.772980
318.940995	14068.857558	28.777997
319.188774	14091.342758	28.783015
319.282065	14110.337432	28.788032
319.352957	14128.944981	28.793050
320.051150	14151.341528	28.798068
320.664418	14176.768697	28.803085
320.584331	14200.458821	28.808103
321.006727	14204.880662	28.813120
321.214394	14227.158346	28.818138
321.614648	14249.166202	28.823156
321.903528	14262.708665	28.828173
322.265498	14285.567666	28.833191
322.817043	14292.609612	28.838208
322.899864	14323.160283	28.843226
323.193028	14317.921864	28.848244
323.582772	14342.609296	28.853261
323.851373	14354.311209	28.858279
324.557087	14366.938425	28.863296
324.177421	14387.434881	28.868314
324.547553	14407.515689	28.873332
325.035847	14422.591882	28.878349
325.323473	14453.050582	28.883367
325.869263	14467.389159	28.888384
325.495015	14494.042539	28.893402
326.021365	14521.073308	28.898420
326.507771	14541.730790	28.903437
326.722663	14571.273442	28.908455
327.122122	14596.103071	28.913472
327.098896	14631.508851	28.918490
327.632489	14648.530519	28.923508
328.190368	14676.178879	28.928525
328.176142	14701.939257	28.933543
328.598716	14726.877161	28.938560
328.694108	14759.622056	28.943578
328.908936	14792.459152	28.948596
329.659653	14807.664061	28.953613
329.720288	14846.928897	28.958631
330.257308	14865.797416	28.963648
330.794879	14891.977421	28.968666
330.944578	14914.450037	28.973684
331.452658	14943.643796	28.978701
332.096820	14967.193086	28.983719
332.253487	14982.143431	28.988736
332.779942	15009.688803	28.993754
332.866001	15033.108329	28.998772
333.285232	15048.122452	29.003789
333.251660	15079.563813	29.008807
333.898411	15104.471491	29.013824
334.136715	15129.052778	29.018842
334.256984	15159.237872	29.023860
334.896518	15188.700318	29.028877
335.219667	15219.012707	29.033895
335.507931	15235.599599	29.038912
336.134727	15261.696076	29.043930
335.935447	15286.506061	29.048948
336.601272	15304.403353	29.053965
336.955607	15340.958648	29.058983
337.558827	15356.161687	29.064000
337.720922	15377.904703	29.069018
337.974528	15398.631744	29.074036
338.670065	15414.476815	29.079053
338.524104	15447.910827	29.084071
339.078850	15454.495663	29.089088
339.152060	15490.683290	29.094106
339.206196	15518.247794	29.099124
340.017305	15543.412646	29.104141
339.980775	15576.781523	29.109159
340.584157	15590.477932	29.114176
341.112195	15618.700242	29.119194
341.516575	15647.945516	29.124212
342.214131	15661.232354	29.129229
342.376374	15693.137396	29.134247
342.472222	15700.616323	29.139264
342.775679	15722.946381	29.144282
343.071441	15756.296875	29.149300
343.548077	15772.834217	29.154317
343.646905	15792.086838	29.159335
344.062003	15812.607986	29.164352
344.195373	15837.325913	29.169370
344.265829	15861.403320	29.174388
344.403744	15890.094171	29.179405
344.822677	15920.456624	29.184423
345.582684	15951.875484	29.189440
345.866156	15968.407164	29.194458
346.373794	15999.940391	29.199476
346.674702	16013.208049	29.204493
347.144753	16046.765139	29.209511
347.125558	16057.699421	29.214528
347.451873	16085.169385	29.219546
347.807101	16114.820831	29.224564
348.374106	16135.455948	29.229581
348.464660	16167.728422	29.234599
349.120854	16194.388957	29.239616
349.350850	16223.451324	29.244634
349.620010	16257.845972	29.249652
350.001918	16284.285665	29.254669
349.824651	16307.495232	29.259687
350.555004	16341.884654	29.264704
351.169913	16373.145489	29.269722
351.567332	16403.556527	29.274740
351.905358	16412.338660	29.279757
351.975495	16452.713849	29.284775
352.672655	16491.262510	29.289792
353.051469	16508.029577	29.294810
353.188917	16530.415000	29.299828
353.850780	16546.760110	29.304845
353.793890	16579.516483	29.309863
353.871054	16616.911766	29.314880
354.697623	16643.834863	29.319898
355.033991	16677.654955	29.324916
355.498603	16696.017391	29.329933
355.809131	16740.566889	29.334951
356.366917	16762.756955	29.339968
356.813135	16779.771653	29.344986
356.740359	16816.156582	29.350004
357.584414	16837.528564	29.355021
357.777394	16867.920698	29.360039
358.162564	16887.053116	29.365056
358.869666	16916.486981	29.370074
358.923016	16944.936721	29.375092
359.562712	16959.771084	29.380109
359.449930	16997.364173	29.385127
360.029457	17014.259319	29.390144
360.693760	17038.766640	29.395162
360.421916	17065.527009	29.400180
360.932879	17081.394780	29.405197
361.093535	17116.854268	29.410215
361.603530	17147.924283	29.415232
362.146362	17170.604456	29.420250
362.244000	17190.721150	29.425268
362.730694	17222.606969	29.430285
362.825645	17263.243272	29.435303
363.093989	17293.161847	29.440320
363.625627	17322.430009	29.445338
364.049650	17355.857080	29.450356
364.557652	17373.511617	29.455373
364.882739	17405.134487	29.460391
365.267702	17436.903565	29.465408
365.635494	17454.606616	29.470426
365.941349	17484.071643	29.475444
366.462921	17515.988510	29.480461
366.699713	17544.375812	29.485479
367.235874	17575.434417	29.490496
367.718269	17596.449504	29.495514
367.894709	17621.739914	29.500532
368.339677	17639.580144	29.505549
368.825018	17658.212931	29.510567
368.702007	17686.544950	29.515584
369.522006	17703.894407	29.520602
369.619237	17724.795273	29.525620
369.476660	17746.996956	29.530637
370.324455	17774.621450	29.535655
370.411993	17818.033189	29.540672
371.090870	17836.813853	29.545690
371.278393	17861.128587	29.550708
371.709129	17890.963036	29.555725
371.786881	17930.678474	29.560743
372.113813	17960.486088	29.565760
372.978973	17985.776568	29.570778
372.600454	18021.300421	29.575796
373.457997	18052.385548	29.580813
373.578941	18085.752324	29.585831
373.855753	18122.671828	29.590848
374.589544	18154.094486	29.595866
374.924135	18197.061185	29.600884
375.350266	18214.085412	29.605901
375.786165	18249.050903	29.610919
376.145823	18274.644609	29.615936
376.703889	18304.342070	29.620954
376.585469	18347.111408	29.625972
377.078653	18366.516144	29.630989
377.618293	18396.828478	29.636007
377.899463	18434.662286	29.641024
378.444766	18464.064197	29.646042
378.529663	18501.903842	29.651060
379.528969	18527.467744	29.656077
379.909194	18554.650692	29.661095
380.450426	18589.752381	29.666112
381.094978	18613.489684	29.671130
381.052182	18641.652402	29.676148
381.424201	18669.776468	29.681165
381.790660	18696.424351	29.686183
382.099656	18732.357739	29.691200
382.798431	18744.541763	29.696218
382.930785	18777.401986	29.701236
383.475666	18799.642634	29.706253
383.960528	18821.149147	29.711271
383.814868	18853.276750	29.716288
384.967343	18882.873715	29.721306
384.689370	18914.072712	29.726324
385.260353	18942.134355	29.731341
385.503127	18962.620138	29.736359
385.633481	18997.715014	29.741376
386.382129	19033.543182	29.746394
386.617702	19067.816777	29.751412
386.926653	19097.924207	29.756429
387.123927	19117.875393	29.761447
387.424130	19163.634382	29.766464
388.066856	19200.082665	29.771482
388.241008	19228.078037	29.776500
388.809350	19264.631785	29.781517
389.847247	19298.902345	29.786535
389.889003	19322.898074	29.791552
390.281471	19353.293258	29.796570
390.807314	19382.056784	29.801588
391.233872	19408.081009	29.806605
391.547648	19425.779332	29.811623
391.715325	19467.583485	29.816640
392.289917	19488.298774	29.821658
392.432899	19523.277574	29.826676
393.065982	19542.903317	29.831693
393.336782	19573.013186	29.836711
393.878057	19606.362306	29.841728
394.291116	19625.699790	29.846746
394.519259	19665.818552	29.851764
395.258049	19678.471185	29.856781
395.500415	19703.752263	29.861799
395.788767	19722.448341	29.866816
396.411056	19741.037149	29.871834
396.397773	19770.801823	29.876852
396.878854	19796.656819	29.881869
397.249231	19817.262845	29.886887
397.652568	19856.295189	29.891904
398.015051	19868.419029	29.896922
398.397346	19912.181566	29.901940
398.613752	19933.995654	29.906957
399.000537	19960.735207	29.911975
398.951148	20003.035404	29.916992
399.758563	20026.268482	29.922010
400.072585	20070.615034	29.927028
400.291163	20107.829191	29.932045
401.243073	20138.161593	29.937063
401.334995	20184.068199	29.942080
401.811508	20206.326766	29.947098
402.239640	20251.894126	29.952116
402.460376	20280.892578	29.957133
403.031979	20314.022090	29.962151
403.403794	20350.520866	29.967168
404.004362	20380.500354	29.972186
404.410036	20422.567055	29.977204
404.662847	20452.649946	29.982221
405.493639	20478.683037	29.987239
405.256026	20522.160324	29.992256
405.646959	20548.389296	29.997274
405.897319	20588.418291	30.002292
406.394245	20627.529960	30.007309
406.997200	20671.322598	30.012327
407.346834	20709.177013	30.017344
407.882353	20738.699639	30.022362
408.341401	20780.102510	30.027380
408.787709	20807.103169	30.032397
409.139852	20847.391852	30.037415
409.764776	20886.667410	30.042432
410.358779	20916.727775	30.047450
410.567614	20960.740904	30.052468
410.836371	20989.360532	30.057485
411.359449	21033.280851	30.062503
411.824986	21052.245504	30.067520
412.359879	21080.185838	30.072538
412.633205	21112.111239	30.077556
412.922293	21153.863225	30.082573
413.030908	21189.667905	30.087591
413.975464	21233.332943	30.092608
414.381196	21264.330115	30.097626
414.638927	21295.768089	30.102644
414.919871	21330.696278	30.107661
415.352742	21356.678331	30.112679
415.327257	21408.446282	30.117696
416.399291	21435.823719	30.122714
416.418164	21478.847917	30.127732
417.060053	21515.626173	30.132749
417.733397	21544.526668	30.137767
418.105605	21585.595852	30.142784
418.503982	21617.369068	30.147802
418.825338	21648.426634	30.152820
419.344123	21681.957035	30.157837
419.660411	21707.437018	30.162855
420.175157	21745.974396	30.167872
420.764437	21777.817233	30.172890
420.871737	21815.942864	30.177908
421.291418	21849.314978	30.182925
421.804548	21875.451684	30.187943
421.957333	21907.764346	30.192960
422.392739	21934.729196	30.197978
423.188661	21969.961367	30.202996
423.040064	22006.494661	30.208013
423.889857	22038.230229	30.213031
424.187445	22074.962614	30.218048
424.544134	22097.394883	30.223066
424.875271	22130.266595	30.228084
425.282233	22166.151687	30.233101
425.731990	22204.295627	30.238119
425.983677	22246.838590	30.243136
426.460579	22278.365109	30.248154
426.548004	22313.701054	30.253172
427.372899	22362.420404	30.258189
427.774504	22393.972213	30.263207
428.015966	22436.515767	30.268224
428.550042	22473.924178	30.273242
428.889576	22506.706928	30.278260
429.017676	22560.457119	30.283277
429.855827	22597.418121	30.288295
430.028868	22652.413170	30.293312
430.738010	22694.096284	30.298330
430.855853	22733.674502	30.303348
431.537084	22775.796068	30.308365
432.391044	22799.689132	30.313383
432.578838	22852.944699	30.318400
432.971867	22883.770330	30.323418
433.810764	22916.119593	30.328436
434.395344	22958.036845	30.333453
434.863776	22991.090920	30.338471
435.027186	23025.699871	30.343488
435.340049	23061.050522	30.348506
435.911886	23104.230167	30.353524
436.206760	23147.987165	30.358541
436.716454	23177.325944	30.363559
437.278096	23214.073863	30.368576
437.825006	23248.220849	30.373594
437.863602	23286.935138	30.378612
438.298838	23325.407263	30.383629
438.948297	23364.110520	30.388647
439.076105	23407.134186	30.393664
439.664191	23432.745241	30.398682
440.480230	23477.252601	30.403700
440.699684	23520.422233	30.408717
441.153229	23556.248935	30.413735
441.601471	23595.320324	30.418752
442.221248	23623.736502	30.423770
442.651501	23664.824763	30.428788
442.850045	23709.963190	30.433805
443.346512	23749.629341	30.438823
443.654612	23781.356892	30.443840
444.303863	23823.445345	30.448858
444.774449	23859.832835	30.453876
445.127567	23901.327091	30.458893
445.542349	23936.468725	30.463911
445.735709	23984.035668	30.468928
446.419594	24021.753854	30.473946
447.037320	24065.768863	30.478964
447.567883	24100.289273	30.483981
447.983901	24127.817482	30.488999
448.355064	24164.190535	30.494016
448.887808	24187.425918	30.499034
449.042881	24235.807310	30.504052
450.063350	24273.747902	30.509069
450.543110	24291.308735	30.514087
450.550388	24331.145502	30.519104
451.061831	24368.290578	30.524122
451.570254	24408.574464	30.529140
452.092956	24433.619085	30.534157
452.375662	24455.435907	30.539175
452.929886	24501.749203	30.544192
453.183019	24530.667552	30.549210
453.525635	24563.816461	30.554228
453.882063	24600.006791	30.559245
454.459080	24622.339694	30.564263
454.991205	24674.984117	30.569280
455.093223	24709.810074	30.574298
455.802952	24750.294851	30.579316
456.078098	24783.896920	30.584333
456.154238	24829.331380	30.589351
456.628310	24871.836201	30.594368
457.326688	24914.351321	30.599386
457.639424	24966.900473	30.604404
458.050669	25011.447278	30.609421
458.778133	25057.679789	30.614439
458.913501	25099.503160	30.619456
459.302030	25141.243735	30.624474
459.710377	25187.472630	30.629492
459.874042	25243.788109	30.634509
460.587597	25293.849544	30.639527
461.245836	25345.115710	30.644544
461.739670	25393.494773	30.649562
462.538020	25441.167509	30.654580
463.169106	25486.609652	30.659597
463.620410	25523.694637	30.664615
464.021515	25575.000885	30.669632
464.465990	25611.412189	30.674650
465.048107	25645.409889	30.679668
465.277023	25699.227377	30.684685
466.219108	25743.114163	30.689703
466.684463	25783.531419	30.694720
467.257249	25815.222088	30.699738
467.505436	25858.381809	30.704756
467.937842	25904.463552	30.709773
468.598417	25932.263309	30.714791
468.725516	25980.080161	30.719808
469.217719	26015.945039	30.724826
470.004732	26059.599643	30.729844
470.287603	26109.819889	30.734861
470.408647	26142.683615	30.739879
471.220771	26190.807218	30.744896
471.840046	26236.458326	30.749914
471.913883	26276.928910	30.754932
472.540933	26327.903501	30.759949
473.419228	26361.758975	30.764967
473.536593	26407.070907	30.769984
474.111538	26455.023152	30.775002
474.839374	26483.866231	30.780020
475.011156	26530.308211	30.785037
475.552567	26562.598472	30.790055
475.754167	26611.325824	30.795072
476.422337	26653.396008	30.800090
477.099469	26694.676207	30.805108
477.157912	26741.216368	30.810125
478.010736	26785.735697	30.815143
478.490720	26826.257071	30.820160
478.917078	26860.295561	30.825178
479.247804	26902.917440	30.830196
479.597105	26955.110146	30.835213
480.305105	26988.954024	30.840231
480.777485	27037.811265	30.845248
481.054586	27080.824147	30.850266
481.895581	27119.646136	30.855284
482.319843	27167.902889	30.860301
482.483658	27199.102274	30.865319
483.039146	27240.148390	30.870336
483.486417	27292.701288	30.875354
484.006723	27324.251996	30.880372
484.634977	27359.412617	30.885389
484.847101	27397.967058	30.890407
485.146606	27444.762590	30.895424
485.513354	27481.730127	30.900442
485.928637	27528.263824	30.905460
486.103583	27572.809022	30.910477
486.774368	27625.048338	30.915495
487.195149	27679.237711	30.920512
487.438857	27725.879193	30.925530
488.257151	27767.665411	30.930548
488.674698	27819.729548	30.935565
489.233393	27870.653746	30.940583
490.337953	27927.169274	30.945600
490.690078	27972.086816	30.950618
491.377780	28013.586080	30.955636
491.882089	28069.734509	30.960653
492.318202	28100.716948	30.965671
492.746126	28152.417577	30.970688
493.313571	28197.937317	30.975706
493.750512	28238.059002	30.980724
493.939072	28285.007649	30.985741
494.598220	28327.919388	30.990759
495.401825	28381.148506	30.995776
495.325611	28428.273851	31.000794
496.232269	28467.132159	31.005812
496.878823	28521.949291	31.010829
497.662775	28569.651966	31.015847
497.719000	28608.061372	31.020864
498.427509	28658.679157	31.025882
499.048035	28698.443427	31.030900
499.657641	28738.455669	31.035917
500.165377	28778.743552	31.040935
500.541615	28819.286743	31.045952
500.832291	28871.516983	31.050970
501.449014	28903.631935	31.055988
502.041817	28950.417682	31.061005
502.347154	28990.187450	31.066023
503.314466	29036.782110	31.071040
503.269301	29092.800761	31.076058
503.683549	29135.701380	31.081076
504.021442	29188.325420	31.086093
504.868033	29226.365632	31.091111
505.436435	29279.292530	31.096128
505.313728	29328.128474	31.101146
506.346299	29378.328755	31.106164
506.646635	29434.319721	31.111181
507.323470	29492.551660	31.116199
507.923325	29532.680912	31.121216
508.033553	29590.612567	31.126234
508.857255	29621.009852	31.131252
509.144767	29678.697926	31.136269
509.568045	29738.310340	31.141287
510.470125	29785.507770	31.146304
511.118969	29833.267802	31.151322
512.059518	29878.935261	31.156340
511.991757	29931.467752	31.161357
512.710982	29971.701303	31.166375
513.257124	30004.533525	31.171392
513.804395	30055.958169	31.176410
514.601854	30089.077086	31.181428
514.868402	30141.302484	31.186445
515.396394	30176.072069	31.191463
516.246136	30215.663040	31.196480
516.166358	30257.310408	31.201498
516.924667	30290.783242	31.206516
517.612985	30327.687820	31.211533
517.618838	30376.896633	31.216551
518.355347	30408.404528	31.221568
518.338357	30447.628315	31.226586
519.093439	30489.523011	31.231604
519.470711	30532.086103	31.236621
520.284890	30579.877603	31.241639
520.989532	30620.364309	31.246656
521.119827	30679.400525	31.251674
521.806257	30707.203648	31.256692
522.245690	30755.821178	31.261709
522.379371	30797.100055	31.266727
523.011199	30847.377166	31.271744
523.437181	30905.989749	31.276762
523.878144	30951.016974	31.281780
524.322262	31007.730628	31.286797
525.058257	31059.085960	31.291815
525.551452	31111.301973	31.296832
525.720761	31167.979578	31.301850
526.414376	31219.137299	31.306868
526.815071	31276.912850	31.311885
527.355599	31326.638492	31.316903
528.164715	31386.000173	31.321920
528.424121	31446.046202	31.326938
529.532833	31493.488540	31.331956
529.780315	31561.216890	31.336973
530.041969	31611.787767	31.341991
530.872711	31671.014305	31.347008
531.383286	31731.455177	31.352026
531.847006	31784.719313	31.357044
532.512794	31830.601383	31.362061
533.332056	31883.103345	31.367079
533.972812	31935.909516	31.372096
534.713262	31990.176061	31.377114
535.174345	32033.542991	31.382132
535.549034	32081.199869	31.387149
536.313306	32131.676444	31.392167
536.756456	32178.400881	31.397184
537.329192	32243.165582	31.402202
537.701579	32279.451264	31.407220
538.206139	32327.137801	31.412237
538.969958	32383.916564	31.417255
539.465846	32430.841198	31.422272
539.466414	32481.511399	31.427290
540.457151	32540.758550	31.432308
540.843877	32588.582039	31.437325
541.321865	32641.054362	31.442343
542.308410	32697.077824	31.447360
542.602588	32751.322721	31.452378
543.141512	32797.805744	31.457396
543.706360	32849.778363	31.462413
544.114768	32901.373111	31.467431
544.739709	32958.703665	31.472448
545.309095	33008.126319	31.477466
546.134798	33054.966474	31.482484
546.338414	33112.622837	31.487501
546.764194	33160.450869	31.492519
547.498873	33205.807584	31.497536
547.750874	33276.328106	31.502554
548.240590	33315.701598	31.507572
548.993559	33371.567032	31.512589
549.190442	33439.430824	31.517607
549.994229	33486.414590	31.522624
550.492505	33551.518251	31.527642
551.328729	33607.080327	31.532660
551.815469	33658.493901	31.537677
552.045206	33717.514298	31.542695
552.744983	33764.149948	31.547712
553.156145	33813.048769	31.552730
553.592394	33867.106300	31.557748
554.245568	33912.096459	31.562765
554.607907	33969.902891	31.567783
555.159853	34010.630892	31.572800
555.622422	34075.982207	31.577818
556.569846	34134.017403	31.582836
557.252864	34183.531808	31.587853
557.422177	34238.985295	31.592871
558.213625	34283.944045	31.597888
558.597169	34348.488928	31.602906
559.266047	34396.257956	31.607924
560.043651	34438.221380	31.612941
560.344307	34509.246797	31.617959
560.806335	34561.370802	31.622976
561.596787	34619.215794	31.627994
562.109318	34669.813801	31.633012
562.777158	34730.210425	31.638029
563.423429	34780.761371	31.643047
564.202965	34834.219058	31.648064
564.495402	34891.806496	31.653082
565.112593	34941.179250	31.658100
565.885537	34994.884667	31.663117
566.080673	35054.719947	31.668135
566.915360	35107.462400	31.673152
567.506640	35162.848923	31.678170
568.041572	35221.429283	31.683188
568.705006	35277.507996	31.688205
569.070385	35332.840897	31.693223
569.578222	35387.392965	31.698240
570.031850	35444.611502	31.703258
570.553254	35496.520102	31.708276
571.360117	35559.474954	31.713293
571.901235	35629.489807	31.718311
572.646282	35673.547632	31.723328
573.203886	35739.217503	31.728346
573.645806	35791.007549	31.733364
574.339668	35843.232623	31.738381
574.983644	35909.166554	31.743399
575.550988	35957.054372	31.748416
575.817300	36020.201265	31.753434
576.539438	36080.927985	31.758452
577.153158	36141.388799	31.763469
577.397520	36202.617896	31.768487
578.328907	36263.885023	31.773504
579.055432	36319.101231	31.778522
579.440030	36382.292941	31.783540
580.233597	36429.964684	31.788557
580.486956	36498.998459	31.793575
581.174186	36556.841510	31.798592
581.895802	36621.436447	31.803610
582.356436	36675.132267	31.808628
583.029675	36735.796687	31.813645
583.483728	36792.113593	31.818663
584.259998	36854.030160	31.823680
584.900642	36920.757389	31.828698
585.169114	36974.422765	31.833716
585.780015	37028.492458	31.838733
586.432478	37095.871721	31.843751
586.886800	37152.435891	31.848768
587.826941	37222.592895	31.853786
588.124681	37275.736689	31.858804
589.015385	37330.297559	31.863821
589.575979	37397.604765	31.868839
590.013642	37452.079985	31.873856
590.846974	37508.027042	31.878874
591.414789	37569.522872	31.883892
591.902303	37626.032524	31.888909
592.725933	37673.986642	31.893927
593.142459	37721.481127	31.898944
593.554087	37765.681283	31.903962
594.026663	37822.607503	31.908980
594.764288	37872.312390	31.913997
594.902702	37929.556213	31.919015
595.641119	37987.502676	31.924032
596.386584	38046.129946	31.929050
596.559085	38115.221116	31.934068
597.630747	38173.302423	31.939085
598.249905	38234.927735	31.944103
598.533925	38284.102754	31.949120
599.062777	38344.064132	31.954138
599.496780	38412.122025	31.959156
600.097069	38470.042372	31.964173
600.602312	38552.668903	31.969191
600.899434	38610.308418	31.974208
601.812367	38687.432565	31.979226
602.281387	38768.017467	31.984244
603.190712	38831.269759	31.989261
603.615222	38889.580367	31.994279
604.747239	38948.888381	31.999296
605.313882	39027.911548	32.004314
605.721644	39086.178204	32.009332
606.418292	39154.870922	32.014349
607.101717	39227.129926	32.019367
607.547658	39293.768637	32.024384
608.547253	39352.241262	32.029402
609.190915	39417.269382	32.034420
610.053240	39471.506753	32.039437
610.791245	39532.586455	32.044455
611.421038	39588.093751	32.049472
612.141453	39639.368863	32.054490
612.363137	39702.744249	32.059508
613.326124	39753.553391	32.064525
613.477050	39825.138923	32.069543
614.350398	39884.941024	32.074560
615.019363	39942.217004	32.079578
615.364042	40010.374530	32.084596
616.748020	40072.394047	32.089613
617.037220	40127.211165	32.094631
617.440218	40182.666234	32.099648
618.025797	40231.471436	32.104666
618.288684	40297.051817	32.109684
619.023976	40355.902835	32.114701
619.862807	40426.625571	32.119719
620.188555	40487.334694	32.124736
621.196123	40555.441390	32.129754
621.383166	40618.702541	32.134772
622.096883	40682.754388	32.139789
622.565923	40752.371505	32.144807
623.536091	40805.190155	32.149824
624.208412	40873.596573	32.154842
624.732505	40936.266373	32.159860
625.444733	41000.518456	32.164877
625.857386	41062.332649	32.169895
626.649948	41115.241552	32.174912
627.554025	41193.858305	32.179930
628.357131	41253.837480	32.184948
628.563270	41311.374234	32.189965
629.246366	41373.725611	32.194983
629.947422	41435.262876	32.200000
630.837814	41485.375326	32.205018
631.043573	41552.292404	32.210036
631.914350	41607.500726	32.215053
632.136016	41682.949132	32.220071
632.963487	41747.478351	32.225088
633.619668	41803.130020	32.230106
633.799946	41865.951404	32.235124
634.913289	41911.971270	32.240141
635.298323	41978.402447	32.245159
635.941426	42038.208580	32.250176
636.824439	42091.556779	32.255194
637.153660	42156.659207	32.260212
637.596246	42209.322896	32.265229
638.424569	42272.284700	32.270247
638.864940	42333.587087	32.275264
639.796553	42386.587121	32.280282
639.984048	42461.681266	32.285300
641.016055	42513.907329	32.290317
641.094863	42585.875389	32.295335
641.968685	42650.472695	32.300352
642.980944	42721.762753	32.305370
643.349496	42790.643255	32.310388
644.049298	42859.134541	32.315405
644.786417	42920.042468	32.320423
645.421262	42996.580247	32.325440
645.828073	43067.810772	32.330458
646.495468	43137.110392	32.335476
647.145182	43201.528831	32.340493
648.064810	43269.562178	32.345511
648.913557	43353.814109	32.350528
649.433200	43413.117809	32.355546
649.769839	43482.381866	32.360564
650.711038	43549.591751	32.365581
651.182715	43622.228161	32.370599
651.952587	43692.753741	32.375616
652.724000	43760.788138	32.380634
653.119487	43835.449247	32.385652
653.938519	43905.894877	32.390669
654.550397	43980.814409	32.395687
655.324655	44055.596865	32.400704
656.237784	44119.633884	32.405722
656.517220	44185.683074	32.410740
657.234043	44254.075616	32.415757
657.993834	44333.360998	32.420775
658.639487	44399.366141	32.425792
659.387678	44468.720477	32.430810
659.290431	44544.605789	32.435828
660.488917	44614.198763	32.440845
661.270567	44691.906425	32.445863
661.946276	44774.469341	32.450880
662.758138	44826.252027	32.455898
663.109694	44900.160500	32.460916
664.165551	44975.035810	32.465933
664.765268	45046.365085	32.470951
665.418389	45119.018317	32.475968
666.310576	45189.115635	32.480986
666.585193	45263.777152	32.486004
667.418519	45326.593686	32.491021
668.035656	45390.267191	32.496039
668.509945	45463.990214	32.501056
669.444599	45531.527207	32.506074
669.881154	45616.991100	32.511092
670.386305	45685.240714	32.516109
670.942976	45754.470424	32.521127
671.838404	45835.384874	32.526144
672.710105	45918.498244	32.531162
673.058166	45992.458938	32.536180
673.976281	46063.338344	32.541197
674.575564	46135.224417	32.546215
675.178458	46207.722782	32.551232
676.189699	46285.042192	32.556250
676.571596	46359.270293	32.561268
677.411097	46425.771504	32.566285
678.308835	46494.922237	32.571303
678.861609	46562.740824	32.576320
679.938857	46616.088721	32.581338
680.015105	46690.381312	32.586356
680.803944	46739.586740	32.591373
681.474425	46809.082530	32.596391
681.703274	46874.732645	32.601408
682.643585	46941.818996	32.606426
683.049228	47017.697344	32.611444
683.656078	47084.731993	32.616461
684.096019	47167.530676	32.621479
684.932202	47240.559671	32.626496
685.655418	47314.507663	32.631514
686.277143	47392.303402	32.636532
687.123610	47464.810484	32.641549
687.740911	47547.878334	32.646567
688.663827	47628.896943	32.651584
689.393531	47705.201286	32.656602
690.014450	47782.641889	32.661620
690.930858	47844.578237	32.666637
691.678168	47917.905600	32.671655
692.516970	48001.431447	32.676672
693.280153	48067.682586	32.681690
694.049413	48145.854915	32.686708
694.424913	48208.564083	32.691725
695.319044	48279.809435	32.696743
696.058618	48370.970793	32.701760
696.441051	48429.744453	32.706778
697.212064	48504.965057	32.711796
698.020384	48573.591763	32.716813
698.842065	48659.586718	32.721831
699.311138	48731.759946	32.726848
699.909658	48793.913028	32.731866
700.737121	48879.803792	32.736884
701.485040	48955.001559	32.741901
702.271520	49036.910911	32.746919
702.758890	49124.744526	32.751936
703.616481	49191.416623	32.756954
704.043092	49279.459969	32.761972
704.956121	49369.204557	32.766989
705.676749	49432.334382	32.772007
706.323647	49516.602888	32.777024
707.275268	49592.543251	32.782042
707.961018	49673.647643	32.787060
708.535158	49758.068211	32.792077
709.582188	49834.622269	32.797095
710.003042	49914.931357	32.802112
710.847946	49993.045001	32.807130
711.335735	50069.405084	32.812148
711.935427	50149.698199	32.817165
713.297469	50228.308408	32.822183
713.689346	50299.246365	32.827200
714.506875	50376.936537	32.832218
715.363511	50458.916135	32.837236
715.739523	50538.537200	32.842253
716.490816	50620.737055	32.847271
717.017913	50695.343275	32.852288
718.012717	50765.652568	32.857306
718.377129	50847.494136	32.862324
719.243422	50930.080579	32.867341
719.893469	51013.827610	32.872359
720.416670	51096.275681	32.877376
721.471944	51178.705578	32.882394
722.157810	51261.651778	32.887412
722.649137	51359.116136	32.892429
723.777211	51422.652547	32.897447
723.931897	51507.949275	32.902464
724.935351	51591.627703	32.907482
725.725241	51665.511902	32.912500
726.128776	51738.203119	32.917517
726.920954	51810.230159	32.922535
727.319722	51896.391610	32.927552
728.253100	51970.240596	32.932570
728.936879	52054.795174	32.937588
729.338319	52135.315666	32.942605
730.299313	52215.516497	32.947623
730.850522	52305.520914	32.952640
731.942809	52380.956166	32.957658
732.614596	52472.501868	32.962676
733.322006	52557.294786	32.967693
734.236792	52639.520355	32.972711
734.751521	52719.677041	32.977728
735.374447	52804.762989	32.982746
736.135978	52890.805642	32.987764
737.134555	52974.629804	32.992781
737.657948	53056.719698	32.997799
738.276119	53141.826850	33.002816
739.128502	53243.417024	33.007834
739.861451	53331.178499	33.012852
740.640604	53418.566281	33.017869
741.724969	53507.868870	33.022887
742.171401	53597.264752	33.027904
742.816400	53680.329072	33.032922
743.588114	53775.168683	33.037940
744.225828	53862.076385	33.042957
745.073376	53943.351871	33.047975
745.801672	54048.290085	33.052992
746.944426	54134.818497	33.058010
747.452163	54227.555758	33.063028
748.212448	54313.497440	33.068045
749.094412	54402.047784	33.073063
749.409120	54506.336561	33.078080
750.369425	54597.857083	33.083098
751.469820	54684.584467	33.088116
751.624767	54778.185106	33.093133
752.963837	54867.312726	33.098151
753.383052	54971.428708	33.103168
754.609529	55049.644792	33.108186
755.123972	55149.872713	33.113204
756.054323	55242.007753	33.118221
756.708951	55338.106364	33.123239
757.329761	55431.500340	33.128256
758.261414	55516.881823	33.133274
759.528570	55604.918897	33.138292
760.239917	55690.501855	33.143309
760.937817	55779.335241	33.148327
761.729571	55874.529143	33.153344
762.432812	55948.557516	33.158362
763.285915	56042.219244	33.163380
763.744487	56138.297287	33.168397
765.177481	56210.784187	33.173415
765.301945	56306.893032	33.178432
766.132913	56383.530564	33.183450
766.950142	56472.025040	33.188468
767.698622	56559.191653	33.193485
768.560126	56641.291056	33.198503
769.144063	56734.596145	33.203520
769.811496	56834.434425	33.208538
770.731779	56915.223502	33.213556
771.324312	57007.845982	33.218573
772.258398	57100.715715	33.223591
772.763954	57197.852707	33.228608
773.317451	57288.795719	33.233626
774.495378	57381.253588	33.238644
774.955754	57482.658611	33.243661
775.690202	57570.653463	33.248679
776.438362	57663.493368	33.253696
777.301918	57749.123173	33.258714
778.073866	57822.584706	33.263732
778.884551	57916.609806	33.268749
779.539921	58000.688945	33.273767
780.449058	58094.932414	33.278784
780.974330	58180.973906	33.283802
781.912754	58268.160779	33.288820
782.628686	58357.843139	33.293837
783.489901	58442.749540	33.298855
784.224957	58538.211962	33.303872
784.963396	58637.200641	33.308890
785.431393	58720.384791	33.313908
786.408409	58825.673566	33.318925
787.200130	58915.996804	33.323943
787.484040	59020.333201	33.328960
788.282415	59119.636640	33.333978
789.391956	59213.732119	33.338996
790.277331	59325.175209	33.344013
790.728176	59410.836105	33.349031
791.472221	59526.677044	33.354048
792.334368	59631.862620	33.359066
793.670209	59737.621351	33.364084
793.949567	59845.994908	33.369101
795.337773	59942.405055	33.374119
796.219284	60051.109874	33.379136
796.471355	60147.354987	33.384154
797.611181	60250.254200	33.389172
798.109840	60363.580843	33.394189
798.971194	60469.706279	33.399207
799.824519	60569.108852	33.404224
800.450080	60678.156409	33.409242
801.603448	60783.160733	33.414260
802.023785	60880.032469	33.419277
802.785464	60996.624669	33.424295
803.518858	61103.716309	33.429312
803.986567	61217.210825	33.434330
805.450181	61333.372826	33.439348
806.394205	61437.764135	33.444365
807.364439	61545.046453	33.449383
808.204099	61658.020495	33.454400
808.946640	61762.984038	33.459418
810.007722	61868.597024	33.464436
810.588454	61967.969323	33.469453
811.615921	62068.323773	33.474471
812.243923	62187.681736	33.479488
813.420809	62287.291979	33.484506
814.084062	62380.635245	33.489524
814.414598	62498.166932	33.494541
815.344153	62604.709342	33.499559
816.097852	62711.717532	33.504576
817.194901	62816.716318	33.509594
818.130041	62918.506081	33.514612
818.888543	63027.866521	33.519629
819.701546	63126.238884	33.524647
820.917867	63238.571460	33.529664
821.682077	63340.745559	33.534682
822.420411	63436.331502	33.539700
822.878703	63550.257650	33.544717
823.976453	63646.101176	33.549735
824.767680	63752.527006	33.554752
825.334302	63862.637898	33.559770
826.402846	63975.213843	33.564788
827.103599	64081.972393	33.569805
827.984592	64182.456180	33.574823
828.916495	64295.176568	33.579840
829.243932	64396.479905	33.584858
830.581258	64492.787118	33.589876
831.047429	64605.067856	33.594893
831.745302	64703.409859	33.599911
832.733112	64798.884965	33.604928
833.510432	64906.912042	33.609946
834.399918	64988.338773	33.614964
835.214495	65090.860849	33.619981
835.929866	65198.115800	33.624999
837.003726	65301.790825	33.630016
837.262306	65403.989165	33.635034
838.423527	65501.518659	33.640052
838.927037	65602.109662	33.645069
839.900316	65713.263078	33.650087
840.765097	65824.169511	33.655104
841.898893	65933.502142	33.660122
842.489532	66042.722876	33.665140
843.045157	66161.913372	33.670157
843.994280	66266.783375	33.675175
845.044443	66384.344456	33.680192
844.954496	66501.620603	33.685210
846.724449	66615.510936	33.690228
847.472603	66739.009822	33.695245
848.619688	66846.062723	33.700263
849.339853	66961.690131	33.705280
850.238590	67077.130585	33.710298
851.254544	67182.841285	33.715316
851.745198	67310.666282	33.720333
852.383045	67431.070573	33.725351
853.332002	67539.645516	33.730368
854.302688	67672.008640	33.735386
855.196032	67783.173577	33.740404
855.754043	67905.231284	33.745421
856.701153	68028.009336	33.750439
857.728622	68153.499829	33.755456
858.224535	68270.189416	33.760474
859.309522	68392.643293	33.765492
859.853633	68519.929326	33.770509
861.159244	68652.837517	33.775527
862.202805	68764.886904	33.780544
862.958182	68894.062350	33.785562
864.152792	69009.217817	33.790580
865.005026	69140.629660	33.795597
865.766020	69251.704042	33.800615
866.724995	69368.455852	33.805632
867.681459	69500.073974	33.810650
868.661829	69605.733087	33.815668
869.563476	69739.688610	33.820685
870.133211	69854.642160	33.825703
871.254243	69964.263309	33.830720
871.856510	70094.173202	33.835738
873.039779	70199.864927	33.840756
874.196549	70326.017089	33.845773
874.994119	70442.940569	33.850791
875.993769	70551.819691	33.855808
876.603156	70668.889343	33.860826
877.745109	70776.361266	33.865844
878.383242	70901.793199	33.870861
879.444301	71011.379035	33.875879
880.574454	71122.983823	33.880896
880.847710	71245.853880	33.885914
881.767210	71362.003377	33.890932
882.491832	71480.417937	33.895949
883.470667	71599.923024	33.900967
884.285868	71725.134433	33.905984
884.915796	71846.380665	33.911002
886.374290	71957.208251	33.916020
886.911410	72086.913287	33.921037
887.450807	72203.079577	33.926055
888.765040	72328.091795	33.931072
889.518492	72452.381703	33.936090
890.584993	72564.415514	33.941108
891.476734	72670.325665	33.946125
892.299307	72780.269782	33.951143
893.206552	72893.545820	33.956160
893.979941	73007.369475	33.961178
895.271877	73115.941252	33.966196
895.851516	73239.435960	33.971213
896.559741	73347.871435	33.976231
897.320281	73455.394451	33.981248
897.848859	73588.973893	33.986266
899.220773	73698.344837	33.991284
900.024122	73827.225698	33.996301
900.674041	73947.449492	34.001319
901.453129	74069.840788	34.006336
902.227484	74207.102042	34.011354
903.529095	74332.684397	34.016372
904.380522	74463.742961	34.021389
905.056088	74596.728722	34.026407
906.029725	74719.205310	34.031424
907.058852	74856.637202	34.036442
908.058070	74984.278167	34.041460
908.723284	75121.278579	34.046477
909.699635	75239.039470	34.051495
910.573022	75375.014067	34.056512
911.049771	75521.503508	34.061530
912.475709	75640.533032	34.066548
913.221589	75792.185022	34.071565
914.154398	75924.206511	34.076583
915.381644	76054.617857	34.081600
916.029403	76198.408087	34.086618
917.168182	76333.250484	34.091636
918.385402	76476.967323	34.096653
918.822454	76613.299990	34.101671
920.311918	76745.632796	34.106688
920.846883	76872.393704	34.111706
921.749440	77012.826400	34.116724
923.061307	77144.596389	34.121741
923.670269	77279.279139	34.126759
924.715291	77410.601465	34.131776
925.292730	77554.918115	34.136794
926.584244	77691.293185	34.141812
927.948423	77832.964051	34.146829
928.486207	77963.829532	34.151847
929.460486	78107.040430	34.156864
930.358410	78234.381595	34.161882
931.101405	78377.727353	34.166900
932.401944	78508.033416	34.171917
933.184876	78647.775056	34.176935
934.086804	78785.429405	34.181952
934.845263	78921.881142	34.186970
936.215416	79064.710079	34.191988
936.817477	79203.365430	34.197005
937.636019	79343.516676	34.202023
939.064028	79473.086114	34.207040
939.729549	79620.418893	34.212058
940.603536	79763.290026	34.217076
941.734925	79893.745949	34.222093
942.365963	80041.099824	34.227111
943.410789	80170.673369	34.232128
944.446803	80317.936771	34.237146
945.490218	80455.280582	34.242164
946.171275	80596.911004	34.247181
947.125065	80739.287982	34.252199
948.250323	80878.948854	34.257216
949.028778	81022.077785	34.262234
950.049476	81153.501871	34.267252
951.271864	81288.992824	34.272269
952.036036	81432.790961	34.277287
953.171427	81560.200161	34.282304
953.926601	81690.722291	34.287322
954.829757	81820.619679	34.292340
955.793849	81952.120990	34.297357
956.562478	82091.127035	34.302375
957.665843	82210.213086	34.307392
958.137802	82353.154302	34.312410
959.135759	82477.775990	34.317428
960.156492	82631.130445	34.322445
960.896932	82776.737728	34.327463
961.717599	82911.792251	34.332480
962.616375	83054.009260	34.337498
963.948898	83199.660500	34.342516
964.869535	83344.678486	34.347533
965.515721	83492.880926	34.352551
966.603605	83639.290341	34.357568
967.790230	83794.308081	34.362586
968.639689	83937.171387	34.367604
969.566487	84082.838345	34.372621
970.688852	84239.881712	34.377639
971.874943	84386.222668	34.382656
972.457994	84538.605524	34.387674
973.701983	84703.597891	34.392692
974.744778	84849.326405	34.397709
975.833665	85005.298513	34.402727
976.425732	85146.611000	34.407744
977.600593	85309.474107	34.412762
978.524877	85456.712962	34.417780
979.788204	85615.646873	34.422797
980.596151	85775.985951	34.427815
981.678385	85913.571024	34.432832
982.528792	86073.955742	34.437850
983.558812	86230.477282	34.442868
984.933620	86375.502335	34.447885
985.414081	86539.773351	34.452903
986.852415	86682.113149	34.457920
987.748552	86845.235510	34.462938
988.511866	87003.293340	34.467956
989.810736	87157.720032	34.472973
990.946486	87319.325316	34.477991
991.613802	87463.189478	34.483008
992.783133	87625.556993	34.488026
993.717012	87776.839763	34.493044
994.773537	87931.798849	34.498061
995.739245	88108.460639	34.503079
996.814034	88256.691972	34.508096
997.809117	88409.949393	34.513114
998.861440	88564.666503	34.518132
1000.271644	88717.515538	34.523149
1000.859775	88884.107517	34.528167
1001.892920	89031.281063	34.533184
1003.046760	89187.504256	34.538202
1003.734451	89342.989170	34.543220
1005.181662	89491.381774	34.548237
1005.804936	89655.422914	34.553255
1006.796676	89810.632763	34.558272
1007.882992	89968.694868	34.563290
1009.202755	90130.681191	34.568308
1010.091273	90278.462233	34.573325
1010.896142	90436.029678	34.578343
1012.068422	90590.474244	34.583360
1013.225601	90742.238854	34.588378
1013.903779	90899.627754	34.593396
1015.361346	91049.313045	34.598413
1016.227394	91209.470301	34.603431
1017.328946	91351.368369	34.608448
1018.370665	91518.916262	34.613466
1019.357087	91666.278224	34.618484
1020.487154	91816.395832	34.623501
1020.994830	91959.832379	34.628519
1022.310944	92094.490367	34.633536
1022.754256	92239.572148	34.638554
1023.916045	92385.922115	34.643572
1025.225204	92532.761272	34.648589
1025.641439	92678.394467	34.653607
1026.776915	92838.910340	34.658624
1027.727622	92998.299527	34.663642
1028.631729	93149.652655	34.668660
1029.754085	93306.591270	34.673677
1030.578036	93478.549707	34.678695
1031.754364	93638.000697	34.683712
1032.537935	93804.049887	34.688730
1033.269830	93965.741238	34.693748
1034.621065	94125.603225	34.698765
1035.763141	94303.566084	34.703783
1037.067956	94458.988061	34.708800
1037.801037	94632.146938	34.713818
1039.091958	94792.130829	34.718836
1039.916283	94959.276141	34.723853
1041.131119	95146.126653	34.728871
1042.385891	95306.562950	34.733888
1043.306406	95472.562740	34.738906
1044.488757	95651.826314	34.743924
1045.826923	95814.644904	34.748941
1046.599443	95981.280260	34.753959
1047.896106	96154.489517	34.758976
1048.961057	96312.748099	34.763994
1049.661061	96486.083632	34.769012
1050.514428	96656.869179	34.774029
1051.568497	96825.710914	34.779047
1053.158013	97000.390594	34.784064
1054.742240	97162.499933	34.789082
1055.570194	97341.524041	34.794100
1056.514874	97509.609807	34.799117
1057.513487	97672.648576	34.804135
1058.518737	97841.600177	34.809152
1059.885495	98007.878544	34.814170
1060.570465	98181.221935	34.819188
1061.907891	98345.861375	34.824205
1063.031297	98517.469576	34.829223
1064.117466	98671.092649	34.834240
1065.028947	98841.769458	34.839258
1065.947344	99019.859867	34.844276
1067.227664	99188.977584	34.849293
1068.178615	99367.084037	34.854311
1069.203221	99538.417919	34.859328
1070.570103	99712.836621	34.864346
1070.823591	99886.180689	34.869364
1072.510989	100055.933294	34.874381
1073.405317	100230.224731	34.879399
1074.500383	100408.017054	34.884416
1075.945282	100583.156905	34.889434
1076.608999	100759.870674	34.894452
1077.729229	100932.774615	34.899469
1078.938359	101110.381998	34.904487
1079.984800	101285.478551	34.909504
1081.047522	101462.226150	34.914522
1082.345918	101638.480118	34.919540
1083.310234	101809.883469	34.924557
1084.362909	101982.159789	34.929575
1085.275910	102154.979555	34.934592
1086.620867	102329.077733	34.939610
1087.412231	102510.809845	34.944628
1088.745976	102676.421192	34.949645
1089.813107	102858.293768	34.954663
1090.738337	103034.454298	34.959680
1092.099060	103202.945590	34.964698
1092.655351	103362.079206	34.969716
1094.079637	103528.934755	34.974733
1095.243207	103690.034234	34.979751
1095.986368	103856.485248	34.984768
1097.210327	104021.958656	34.989786
1098.111709	104196.946839	34.994804
1099.302931	104362.959721	34.999821
1100.448304	104539.822207	35.004839
1101.674245	104710.289515	35.009856
1102.638253	104880.028675	35.014874
1103.369912	105064.688646	35.019892
1104.157435	105236.181707	35.024909
1105.454835	105411.847061	35.029927
1106.497361	105600.144925	35.034944
1107.774657	105784.403083	35.039962
1108.957619	105973.237653	35.044980
1110.017114	106153.430798	35.049997
1110.973381	106339.557044	35.055015
1112.076670	106529.624630	35.060032
1113.665742	106710.759914	35.065050
1114.313067	106905.528552	35.070068
1115.691116	107086.359295	35.075085
1116.671269	107282.798219	35.080103
1117.884108	107467.547312	35.085120
1119.261511	107666.494589	35.090138
1120.287966	107865.818016	35.095156
1121.294910	108051.795797	35.100173
1122.434971	108237.930185	35.105191
1122.993844	108426.872580	35.110208
1124.365177	108623.699955	35.115226
1125.319907	108825.778327	35.120244
1126.525303	109030.818802	35.125261
1127.905918	109234.248496	35.130279
1128.881659	109443.598808	35.135296
1130.244923	109639.256860	35.140314
1131.394942	109845.870696	35.145332
1132.494751	110033.746808	35.150349
1133.506736	110233.077373	35.155367
1134.879270	110438.822865	35.160384
1136.131510	110635.988512	35.165402
1137.223497	110851.334828	35.170420
1138.330974	111039.292581	35.175437
1139.524825	111249.393397	35.180455
1140.661630	111461.861485	35.185472
1142.013145	111641.789537	35.190490
1142.989473	111853.286396	35.195508
1144.195032	112046.910127	35.200525
1145.490387	112252.124535	35.205543
1146.634364	112457.086783	35.210560
1147.682579	112657.999790	35.215578
1148.882401	112857.647664	35.220596
1149.960635	113058.355903	35.225613
1150.958358	113263.918365	35.230631
1152.011000	113465.393889	35.235648
1153.463867	113665.309766	35.240666
1154.271398	113878.408208	35.245684
1155.727655	114081.886500	35.250701
1156.917845	114281.305424	35.255719
1157.728387	114494.205333	35.260736
1159.113140	114697.750583	35.265754
1160.303707	114906.270512	35.270772
1161.529765	115113.506484	35.275789
1162.546862	115319.929650	35.280807
1163.649257	115527.759236	35.285824
1165.531005	115733.459668	35.290842
1166.196216	115938.019683	35.295860
1167.345319	116137.952623	35.300877
1169.014369	116324.307312	35.305895
1169.690074	116513.234773	35.310912
1170.756580	116690.062089	35.315930
1172.279534	116881.246612	35.320948
1173.249010	117077.845505	35.325965
1174.092101	117265.647930	35.330983
1175.125013	117474.086025	35.336000
1176.665421	117663.448303	35.341018
1177.345175	117866.119081	35.346036
1178.510047	118069.902155	35.351053
1179.709997	118277.368128	35.356071
1180.698566	118481.069206	35.361088
1181.623471	118687.988048	35.366106
1182.945989	118908.008091	35.371124
1183.997928	119117.810720	35.376141
1185.516981	119337.662141	35.381159
1186.722463	119545.744496	35.386176
1187.962305	119756.192251	35.391194
1189.001661	119989.610514	35.396212
1190.696028	120186.769604	35.401229
1191.642128	120401.401572	35.406247
1192.551255	120630.411289	35.411264
1193.879649	120844.007547	35.416282
1194.668792	121072.406929	35.421300
1195.985822	121285.754821	35.426317
1197.461992	121514.588962	35.431335
1198.481071	121748.417360	35.436352
1200.040894	121964.593995	35.441370
1201.141165	122197.994317	35.446388
1202.568410	122417.161569	35.451405
1203.824705	122631.061428	35.456423
1205.045195	122853.396263	35.461440
1206.399029	123080.551821	35.466458
1207.567952	123301.187642	35.471476
1208.600902	123525.028549	35.476493
1209.929929	123753.219833	35.481511
1211.160770	123972.392910	35.486528
1212.603977	124183.979051	35.491546
1214.116500	124407.835958	35.496564
1215.078116	124628.338334	35.501581
1216.591470	124858.357862	35.506599
1217.652142	125083.321027	35.511616
1219.280538	125302.425343	35.516634
1220.460695	125512.543357	35.521652
1221.750341	125722.061708	35.526669
1222.729000	125940.580929	35.531687
1224.135384	126165.266790	35.536704
1225.376304	126369.030792	35.541722
1226.551709	126600.792338	35.546740
1227.738863	126812.198237	35.551757
1229.448448	127027.587813	35.556775
1230.756057	127234.654622	35.561792
1231.711385	127449.284579	35.566810
1232.793506	127666.886358	35.571828
1233.848508	127886.978459	35.576845
1235.490216	128095.897058	35.581863
1236.066207	128328.835338	35.586880
1237.698707	128542.993334	35.591898
1238.778850	128763.822642	35.596916
1240.051660	128984.406179	35.601933
1240.932359	129202.140695	35.606951
1242.102047	129424.696415	35.611968
1243.668358	129661.207561	35.616986
1244.766200	129882.346030	35.622004
1246.003795	130109.560084	35.627021
1247.514579	130326.779918	35.632039
1248.890139	130557.105366	35.637056
1249.960467	130760.900894	35.642074
1251.038876	130974.786731	35.647092
1252.499662	131183.857155	35.652109
1253.604769	131386.383301	35.657127
1254.696100	131605.379850	35.662144
1256.195549	131810.442196	35.667162
1257.615570	132021.058711	35.672180
1258.400769	132226.774200	35.677197
1259.665998	132443.288428	35.682215
1260.541144	132668.501607	35.687232
1262.040116	132889.391784	35.692250
1262.967527	133111.556919	35.697268
1264.090538	133339.269230	35.702285
1265.415855	133554.665375	35.707303
1266.600104	133791.435022	35.712320
1267.974946	134020.555709	35.717338
1268.983458	134260.096148	35.722356
1270.326251	134482.886579	35.727373
1271.628996	134727.110581	35.732391
1272.587208	134976.819476	35.737408
1274.277527	135213.110074	35.742426
1275.663948	135446.878954	35.747444
1276.523052	135697.598582	35.752461
1277.926454	135941.485320	35.757479
1279.306488	136192.211339	35.762496
1280.433265	136440.673636	35.767514
1281.879617	136689.807644	35.772532
1282.806322	136945.926573	35.777549
1284.307727	137190.059839	35.782567
1285.292980	137444.867004	35.787584
1286.711246	137700.492057	35.792602
1287.822919	137948.562326	35.797620
1289.090441	138218.289923	35.802637
1291.037290	138474.226535	35.807655
1292.211572	138737.025482	35.812672
1293.358478	138988.153267	35.817690
1294.680383	139250.488010	35.822708
1295.888651	139513.959359	35.827725
1297.095578	139770.484496	35.832743
1298.591949	140042.306251	35.837760
1299.958971	140299.240000	35.842778
1301.465846	140559.208429	35.847796
1302.714620	140824.521748	35.852813
1304.005141	141076.313150	35.857831
1305.523300	141347.038429	35.862848
1306.771503	141600.019896	35.867866
1308.043042	141860.468132	35.872884
1309.018113	142129.196990	35.877901
1310.703215	142398.127579	35.882919
1311.657930	142663.351368	35.887936
1312.979335	142925.980389	35.892954
1314.714781	143188.340047	35.897972
1315.785002	143472.889275	35.902989
1317.120571	143717.248491	35.908007
1318.381868	143998.257695	35.913024
1319.547826	144256.750182	35.918042
1320.949842	144535.267521	35.923060
1322.227362	144802.673247	35.928077
1323.718224	145068.384424	35.933095
1325.141959	145346.587457	35.938112
1326.172709	145617.248516	35.943130
1327.819530	145881.189846	35.948148
1328.939417	146148.961378	35.953165
1330.723155	146427.202028	35.958183
1331.969308	146691.583272	35.963200
1333.302850	146955.470070	35.968218
1334.703691	147228.022388	35.973236
1336.056133	147489.259312	35.978253
1337.309257	147747.648260	35.983271
1338.424894	148004.945680	35.988288
1339.831086	148246.330808	35.993306
1341.036959	148503.743626	35.998324
1342.210262	148763.205566	36.003341
1343.659704	149012.058769	36.008359
1344.765097	149268.326674	36.013376
1346.475385	149535.479980	36.018394
1347.544017	149787.952591	36.023412
1348.673635	150053.835782	36.028429
1350.326926	150311.415462	36.033447
1351.198965	150578.131308	36.038464
1352.966517	150855.926024	36.043482
1354.325433	151108.663940	36.048500
1355.668029	151391.289201	36.053517
1357.131312	151654.084425	36.058535
1358.312217	151933.645580	36.063552
1359.430090	152188.777049	36.068570
1361.226632	152463.331615	36.073588
1362.449932	152752.265321	36.078605
1364.288626	153015.997233	36.083623
1365.644116	153295.057458	36.088640
1366.530746	153561.791749	36.093658
1367.891025	153831.100675	36.098676
1369.301968	154114.977782	36.103693
1370.853374	154390.575964	36.108711
1372.105633	154678.948436	36.113728
1373.666353	154959.242483	36.118746
1375.137826	155242.369359	36.123764
1376.353762	155532.162139	36.128781
1377.978524	155803.356376	36.133799
1379.000269	156083.607951	36.138816
1380.422971	156364.340714	36.143834
1382.138116	156650.126693	36.148852
1383.651947	156933.410873	36.153869
1385.149284	157212.982883	36.158887
1386.601548	157497.993792	36.163904
1387.651921	157783.745484	36.168922
1389.334872	158055.681168	36.173940
1390.571968	158344.057322	36.178957
1391.793387	158618.635629	36.183975
1393.257548	158921.846474	36.188992
1394.682198	159210.654473	36.194010
1396.560041	159497.892624	36.199028
1397.524167	159781.642765	36.204045
1399.038115	160059.975648	36.209063
1400.502158	160354.037398	36.214080
1401.939993	160644.515221	36.219098
1403.351176	160924.850026	36.224116
1404.618334	161222.274402	36.229133
1406.512941	161500.300289	36.234151
1407.613024	161793.100205	36.239168
1409.069912	162081.301190	36.244186
1410.861943	162366.556068	36.249204
1411.908171	162650.553196	36.254221
1413.496225	162928.829472	36.259239
1414.916404	163226.369566	36.264256
1416.332090	163509.118744	36.269274
1418.276166	163781.340518	36.274292
1419.181258	164068.935639	36.279309
1420.768761	164360.264327	36.284327
1421.873235	164641.080383	36.289344
1423.389325	164934.683190	36.294362
1424.678549	165216.956938	36.299380
1425.890103	165507.378468	36.304397
1427.436370	165794.549173	36.309415
1428.841658	166091.274001	36.314432
1430.311938	166377.078041	36.319450
1431.768709	166663.038425	36.324468
1433.120038	166945.934753	36.329485
1434.763830	167217.681968	36.334503
1435.752729	167483.524596	36.339520
1437.341831	167765.638201	36.344538
1438.843963	168042.057947	36.349556
1439.882808	168318.961996	36.354573
1441.316818	168599.406137	36.359591
1442.887215	168887.366826	36.364608
1444.528697	169174.277080	36.369626
1445.360994	169449.331470	36.374644
1446.718743	169745.047813	36.379661
1448.461365	170037.263622	36.384679
1449.874812	170332.555793	36.389696
1451.289716	170638.445445	36.394714
1452.721013	170925.426753	36.399732
1454.005221	171233.435725	36.404749
1455.310185	171533.689795	36.409767
1456.823722	171834.799622	36.414784
1458.027588	172142.967446	36.419802
1459.975264	172446.953543	36.424820
1461.306072	172756.893706	36.429837
1462.723158	173073.077943	36.434855
1464.404038	173379.385659	36.439872
1465.751186	173683.123564	36.444890
1467.490555	173997.420548	36.449908
1468.606467	174318.117143	36.454925
1470.200827	174628.152772	36.459943
1472.032694	174926.196435	36.464960
1473.221865	175257.153962	36.469978
1475.104547	175563.124904	36.474996
1476.515741	175881.574780	36.480013
1477.875404	176200.657094	36.485031
1479.369334	176513.551368	36.490048
1480.647139	176830.392234	36.495066
1482.434444	177146.909791	36.500084
1483.724497	177468.473859	36.505101
1485.176002	177782.423792	36.510119
1486.926246	178107.901037	36.515136
1488.201596	178438.459359	36.520154
1489.851609	178758.461851	36.525172
1491.245909	179077.429797	36.530189
1492.614336	179409.667040	36.535207
1494.662567	179732.592415	36.540224
1495.685608	180066.413995	36.545242
1497.354679	180385.738088	36.550260
1499.034921	180709.796490	36.555277
1500.704437	181028.946752	36.560295
1502.040026	181353.345310	36.565312
1503.846587	181672.895681	36.570330
1505.507465	182000.112955	36.575348
1506.669401	182316.613272	36.580365
1508.146478	182646.581100	36.585383
1509.832663	182963.557098	36.590400
1511.063558	183296.818938	36.595418
1513.177910	183626.230527	36.600436
1514.706573	183963.788242	36.605453
1516.052680	184288.862840	36.610471
1517.314713	184606.032736	36.615488
1518.830968	184934.675199	36.620506
1520.675818	185249.734275	36.625524
1522.111159	185574.522447	36.630541
1523.427887	185898.177004	36.635559
1524.940982	186211.481163	36.640576
1526.366270	186548.995535	36.645594
1528.318274	186869.656576	36.650612
1530.057177	187195.025927	36.655629
1531.291050	187508.370693	36.660647
1533.007368	187821.447053	36.665664
1533.880571	188136.073443	36.670682
1535.761651	188437.752160	36.675700
1537.116704	188746.285293	36.680717
1538.365630	189051.397482	36.685735
1540.045088	189366.481237	36.690752
1541.370485	189672.878827	36.695770
1543.240393	189997.061663	36.700788
1544.230916	190309.420736	36.705805
1546.208124	190626.404239	36.710823
1547.821015	190946.889830	36.715840
1548.946903	191259.155316	36.720858
1550.433114	191585.415880	36.725876
1552.032132	191910.021934	36.730893
1553.574686	192241.900471	36.735911
1554.984410	192575.872011	36.740928
1556.299607	192911.676352	36.745946
1557.936498	193247.899075	36.750964
1559.325278	193580.952746	36.755981
1560.867068	193932.733644	36.760999
1562.444487	194277.617112	36.766016
1563.760895	194621.771166	36.771034
1565.232641	194978.876072	36.776052
1567.121460	195332.981416	36.781069
1568.475262	195685.044254	36.786087
1570.337937	196051.777184	36.791104
1571.754860	196405.433137	36.796122
1573.602783	196757.153522	36.801140
1575.031114	197118.213022	36.806157
1576.776752	197464.837672	36.811175
1578.217305	197825.873601	36.816192
1579.729385	198185.477706	36.821210
1581.305107	198547.637814	36.826228
1583.477159	198911.059817	36.831245
1584.805161	199272.350584	36.836263
1586.446546	199624.031201	36.841280
1588.436999	199996.630245	36.846298
1590.279377	200350.465106	36.851316
1591.400866	200711.048396	36.856333
1592.789471	201080.464260	36.861351
1595.041679	201430.275527	36.866368
1596.389869	201801.098434	36.871386
1598.122809	202152.357558	36.876404
1600.123947	202526.072747	36.881421
1601.617390	202877.527313	36.886439
1603.317418	203239.665611	36.891456
1604.898475	203596.340261	36.896474
1606.825501	203944.109655	36.901492
1608.229898	204305.768726	36.906509
1609.843495	204663.598535	36.911527
1611.691091	205011.919275	36.916544
1612.935306	205374.524117	36.921562
1614.885827	205727.275154	36.926580
1616.563441	206078.333351	36.931597
1618.084749	206441.570392	36.936615
1619.689537	206792.923182	36.941632
1621.508864	207144.394469	36.946650
1623.202179	207499.646620	36.951668
1624.891441	207864.309981	36.956685
1626.734804	208203.808079	36.961703
1628.277080	208535.345055	36.966720
1629.857915	208903.649872	36.971738
1631.286234	209243.182771	36.976756
1633.338227	209593.686621	36.981773
1634.735790	209942.852489	36.986791
1636.658440	210279.565191	36.991808
1638.244505	210637.997758	36.996826
1639.794653	210979.549256	37.001844
1641.565212	211315.300733	37.006861
1642.800995	211644.157834	37.011879
1644.769180	211971.142829	37.016896
1646.258516	212295.160553	37.021914
1647.873429	212623.247598	37.026932
1649.640776	212946.993215	37.031949
1650.907362	213277.019577	37.036967
1652.665121	213599.854846	37.041984
1654.063828	213946.014326	37.047002
1655.387449	214278.828593	37.052020
1657.034338	214618.168561	37.057037
1658.567060	214971.928948	37.062055
1660.333387	215316.458195	37.067072
1661.902358	215666.303998	37.072090
1663.599739	216020.777651	37.077108
1665.246312	216381.610450	37.082125
1666.684115	216725.919680	37.087143
1668.548070	217086.490611	37.092160
1669.834299	217450.612432	37.097178
1671.478212	217806.752288	37.102196
1673.347632	218180.584121	37.107213
1674.702322	218545.866938	37.112231
1676.362176	218921.310816	37.117248
1678.285585	219299.734952	37.122266
1679.631037	219665.556640	37.127284
1681.278556	220056.829987	37.132301
1682.826583	220442.127103	37.137319
1684.905205	220817.660991	37.142336
1686.590625	221213.402511	37.147354
1688.224879	221580.630785	37.152372
1690.264897	221969.941302	37.157389
1691.593920	222361.478759	37.162407
1693.765024	222740.890006	37.167424
1695.446375	223137.807402	37.172442
1697.366585	223521.631378	37.177460
1698.857143	223891.100640	37.182477
1700.834615	224290.868608	37.187495
1702.502905	224718.654100	37.192512
1704.152123	225128.232586	37.197530
1705.847494	225520.558288	37.202548
1707.572328	225910.949972	37.207565
1709.139521	226292.758295	37.212583
1710.893524	226680.658348	37.217600
1712.696751	227071.294672	37.222618
1714.517189	227463.072344	37.227636
1716.201026	227856.067569	37.232653
1717.807104	228252.150256	37.237671
1720.021531	228643.764734	37.242688
1721.435116	229037.595469	37.247706
1723.190698	229428.627565	37.252724
1725.234501	229818.368511	37.257741
1726.609348	230207.128791	37.262759
1728.456720	230611.535210	37.267776
1730.394111	231001.398545	37.272794
1732.387184	231382.210954	37.277812
1734.081632	231779.533548	37.282829
1735.841267	232177.151227	37.287847
1737.583798	232554.985220	37.292864
1739.398214	232947.210765	37.297882
1741.099810	233333.943826	37.302900
1742.605793	233724.520330	37.307917
1744.226226	234114.672437	37.312935
1745.982018	234508.029090	37.317952
1747.749743	234899.758986	37.322970
1749.252639	235291.711327	37.327988
1751.287868	235689.393604	37.333005
1753.130732	236091.579246	37.338023
1754.830163	236480.275721	37.343040
1756.068051	236876.796809	37.348058
1757.751895	237267.580453	37.353076
1759.419221	237631.060538	37.358093
1761.276498	238015.517371	37.363111
1763.114846	238398.911192	37.368128
1764.572313	238777.847078	37.373146
1766.496748	239167.959679	37.378164
1768.133456	239552.887679	37.383181
1769.321545	239941.573789	37.388199
1771.520969	240337.028372	37.393216
1772.884700	240730.614900	37.398234
1774.465294	241142.430584	37.403252
1776.350275	241545.153463	37.408269
1778.092080	241953.743231	37.413287
1779.960654	242356.165341	37.418304
1781.588962	242765.308643	37.423322
1783.105040	243188.493349	37.428340
1784.919152	243608.377972	37.433357
1786.402575	244040.003079	37.438375
1788.448642	244462.797399	37.443392
1789.974474	244897.109487	37.448410
1791.663849	245335.764472	37.453428
1793.885495	245769.632655	37.458445
1795.477166	246209.575143	37.463463
1797.209471	246643.347498	37.468480
1799.239634	247093.075034	37.473498
1800.328541	247545.981546	37.478516
1802.804043	247995.509639	37.483533
1804.238558	248447.420245	37.488551
1806.128023	248893.438931	37.493568
1808.086501	249357.736881	37.498586
1809.779366	249812.756263	37.503604
1811.667170	250264.187462	37.508621
1813.276036	250711.854680	37.513639
1815.390239	251179.735931	37.518656
1817.482485	251643.226461	37.523674
1819.322199	252100.865529	37.528692
1821.473407	252565.210735	37.533709
1823.165656	253023.332064	37.538727
1824.848876	253468.575736	37.543744
1826.822904	253942.832935	37.548762
1828.689208	254404.813008	37.553780
1830.927982	254858.577341	37.558797
1832.391567	255327.483220	37.563815
1834.100828	255786.466826	37.568832
1836.368017	256241.065281	37.573850
1838.307734	256709.359507	37.578868
1840.452818	257158.567445	37.583885
1842.195292	257624.938368	37.588903
1844.206411	258075.286300	37.593920
1846.373909	258521.594710	37.598938
1847.863234	258988.083735	37.603956
1849.962116	259442.481714	37.608973
1851.739978	259897.085086	37.613991
1853.724953	260347.945309	37.619008
1855.605916	260807.612162	37.624026
1857.586427	261260.987850	37.629044
1859.381692	261704.766156	37.634061
1861.186289	262171.735954	37.639079
1863.489938	262607.554966	37.644096
1865.042087	263061.839040	37.649114
1866.723988	263522.299849	37.654132
1868.833262	263968.997494	37.659149
1870.843259	264427.371341	37.664167
1872.545271	264876.167943	37.669184
1874.423243	265324.655744	37.674202
1875.761129	265789.185580	37.679220
1877.617482	266238.539962	37.684237
1879.274225	266688.409589	37.689255
1881.233062	267133.326134	37.694272
1883.350404	267569.502843	37.699290
1885.084552	268003.176709	37.704308
1886.998875	268437.150628	37.709325
1888.198163	268868.117607	37.714343
1890.001341	269312.727391	37.719360
1891.878002	269770.940488	37.724378
1893.742648	270219.908344	37.729396
1895.360842	270675.140025	37.734413
1896.934890	271152.834474	37.739431
1899.032185	271618.375497	37.744448
1900.566897	272083.907121	37.749466
1902.161999	272558.776252	37.754484
1904.239028	273030.516711	37.759501
1906.023702	273522.550547	37.764519
1907.887260	274005.908197	37.769536
1910.209761	274495.844642	37.774554
1911.957219	274986.662588	37.779572
1913.950282	275477.007170	37.784589
1915.893872	275983.057592	37.789607
1917.464757	276474.460531	37.794624
1919.486496	276981.867594	37.799642
1921.314819	277482.853280	37.804660
1923.507078	277994.903846	37.809677
1925.344820	278502.744160	37.814695
1927.540469	279010.117687	37.819712
1929.328946	279518.547839	37.824730
1931.292486	280038.327802	37.829748
1933.364672	280542.339286	37.834765
1935.156074	281057.623340	37.839783
1937.244373	281577.708628	37.844800
1939.297508	282090.482543	37.849818
1941.138540	282607.252607	37.854836
1943.215311	283130.307134	37.859853
1945.060331	283659.824829	37.864871
1947.128347	284172.488341	37.869888
1949.395511	284694.160148	37.874906
1950.911551	285218.545157	37.879924
1953.293398	285737.832214	37.884941
1955.354312	286265.273368	37.889959
1957.012395	286782.364812	37.894976
1959.134824	287305.397715	37.899994
1960.714474	287850.794690	37.905012
1962.977455	288375.959469	37.910029
1965.097362	288909.528012	37.915047
1967.032331	289440.280140	37.920064
1969.479597	289960.023446	37.925082
1971.473470	290500.337459	37.930100
1973.152435	291019.365158	37.935117
1975.251205	291547.897177	37.940135
1977.396593	292076.012849	37.945152
1979.717685	292601.658852	37.950170
1981.250577	293136.093962	37.955188
1983.551056	293666.132805	37.960205
1985.357596	294185.837051	37.965223
1987.097263	294718.097218	37.970240
1989.366735	295242.876254	37.975258
1991.462716	295774.640795	37.980276
1993.482583	296301.995924	37.985293
1995.332867	296831.890963	37.990311
1997.210199	297372.065357	37.995328
1999.189742	297893.374413	38.000346
2001.320423	298427.888456	38.005364
2003.246297	298952.198036	38.010381
2004.939316	299495.236357	38.015399
2007.092166	300029.128728	38.020416
2009.315297	300565.571785	38.025434
2011.208393	301093.050195	38.030452
2013.566200	301598.861060	38.035469
2014.773324	302106.916407	38.040487
2016.557145	302610.378470	38.045504
2018.678806	303130.010799	38.050522
2020.339296	303658.783053	38.055540
2022.227748	304172.479650	38.060557
2024.309360	304701.938160	38.065575
2026.160518	305233.539468	38.070592
2028.371665	305763.478141	38.075610
2030.029676	306305.593503	38.080628
2032.280494	306850.756671	38.085645
2034.330541	307387.568826	38.090663
2036.243909	307936.183728	38.095680
2038.381677	308481.939037	38.100698
2040.296107	309029.759212	38.105716
2042.017478	309579.867731	38.110733
2044.080090	310144.061178	38.115751
2046.079914	310715.041401	38.120768
2048.135435	311273.209349	38.125786
2050.429735	311840.450480	38.130804
2052.496651	312406.912338	38.135821
2054.396470	312984.723331	38.140839
2056.392468	313570.893990	38.145856
2058.610809	314124.163843	38.150874
2060.596645	314723.125475	38.155892
2062.708068	315301.391288	38.160909
2064.894327	315884.261647	38.165927
2066.976062	316467.423817	38.170944
2069.233525	317056.138546	38.175962
2071.229678	317641.768178	38.180980
2073.392705	318245.520761	38.185997
2075.748523	318822.650736	38.191015
2077.433961	319420.809324	38.196032
2079.779666	319998.438743	38.201050
2081.900790	320600.679058	38.206068
2084.174797	321194.890419	38.211085
2086.393358	321777.527270	38.216103
2088.227098	322378.960708	38.221120
2090.883179	322963.444273	38.226138
2092.633233	323554.800425	38.231156
2094.854723	324155.569025	38.236173
2097.131607	324749.543631	38.241191
2099.190772	325350.835236	38.246208
2101.784803	325925.043898	38.251226
2103.391780	326535.487790	38.256244
2105.571271	327127.271823	38.261261
2108.083177	327721.965547	38.266279
2109.603666	328323.925642	38.271296
2111.840981	328914.945951	38.276314
2114.119897	329522.582299	38.281332
2116.206277	330129.939364	38.286349
2118.459070	330715.353394	38.291367
2120.312634	331318.674242	38.296384
2122.671317	331919.011146	38.301402
2125.005960	332515.791457	38.306420
2126.954318	333128.850764	38.311437
2129.277469	333716.354032	38.316455
2130.795066	334323.327664	38.321472
2133.515113	334926.694345	38.326490
2135.469054	335529.952216	38.331508
2138.177653	336131.504801	38.336525
2140.098009	336728.027609	38.341543
2142.150868	337336.249153	38.346560
2144.530911	337928.290872	38.351578
2146.204737	338529.021958	38.356596
2148.387077	339129.814329	38.361613
2150.706552	339735.551972	38.366631
2152.639503	340325.380505	38.371648
2155.107765	340904.021661	38.376666
2157.203672	341485.966413	38.381684
2159.266005	342048.340571	38.386701
2161.020888	342617.307400	38.391719
2163.013613	343201.583839	38.396736
2165.462176	343778.214488	38.401754
2167.550072	344355.100768	38.406772
2169.284490	344940.870684	38.411789
2171.136252	345524.355161	38.416807
2173.215252	346144.493610	38.421824
2175.681969	346723.369442	38.426842
2177.589393	347331.998209	38.431860
2179.257610	347940.023937	38.436877
2182.023656	348545.398670	38.441895
2183.727857	349177.003595	38.446912
2185.961750	349789.123856	38.451930
2188.335258	350405.958207	38.456948
2190.430605	351039.451668	38.461965
2192.598728	351657.545932	38.466983
2194.981710	352288.791538	38.472000
2197.470314	352924.425912	38.477018
2199.309311	353558.787895	38.482036
2201.722178	354203.246485	38.487053
2204.188148	354836.369537	38.492071
2205.998191	355462.892621	38.497088
2208.301392	356107.467204	38.502106
2210.461591	356750.203195	38.507124
2212.911756	357397.499251	38.512141
2215.131877	358037.439706	38.517159
2217.408570	358691.721469	38.522176
2219.408061	359346.672763	38.527194
2221.618956	360000.030907	38.532212
2223.997614	360652.741835	38.537229
2226.420002	361306.145246	38.542247
2228.186617	361977.050005	38.547264
2230.415736	362634.928487	38.552282
2232.898426	363301.836243	38.557300
2235.073206	363969.620557	38.562317
2237.145361	364637.359538	38.567335
2239.632003	365316.484787	38.572352
2242.083468	365984.670391	38.577370
2244.546140	366663.572609	38.582388
2246.823076	367325.117176	38.587405
2248.934903	367987.159266	38.592423
2250.755241	368664.964387	38.597440
2253.716401	369343.279024	38.602458
2255.887983	370029.599883	38.607476
2257.947171	370702.458004	38.612493
2260.267261	371382.996542	38.617511
2262.098775	372064.718873	38.622528
2264.911484	372739.748075	38.627546
2266.985746	373415.596522	38.632564
2269.321061	374100.214912	38.637581
2271.622995	374778.586629	38.642599
2273.661149	375467.209159	38.647616
2275.658930	376147.075427	38.652634
2278.365346	376833.278148	38.657652
2280.796279	377526.131434	38.662669
2283.348736	378207.615252	38.667687
2285.214210	378910.550477	38.672704
2287.686497	379589.585369	38.677722
2290.015197	380276.617783	38.682740
2292.063661	380974.382868	38.687757
2294.454053	381659.703060	38.692775
2296.646752	382351.989125	38.697792
2299.044204	383040.879943	38.702810
2301.486583	383735.149358	38.707828
2303.505450	384420.168904	38.712845
2305.784461	385078.408387	38.717863
2308.296928	385762.202405	38.722880
2310.335691	386409.882010	38.727898
2312.727463	387072.270367	38.732916
2315.134091	387736.543768	38.737933
2317.452835	388394.936254	38.742951
2319.483498	389066.823483	38.747968
2322.043710	389733.868424	38.752986
2324.237460	390402.303002	38.758004
2325.916815	391084.952562	38.763021
2328.496660	391762.368705	38.768039
2330.420472	392449.459461	38.773056
2332.920129	393142.852430	38.778074
2335.506194	393835.378794	38.783092
2337.300648	394532.860890	38.788109
2339.665142	395233.350109	38.793127
2342.069890	395939.848207	38.798144
2344.310606	396650.563611	38.803162
2346.646899	397361.068682	38.808180
2348.630564	398081.979900	38.813197
2351.143856	398801.797537	38.818215
2353.379278	399531.120871	38.823232
2355.813654	400270.960058	38.828250
2358.076521	400999.810818	38.833268
2360.479284	401743.215450	38.838285
2363.082774	402476.685323	38.843303
2365.600753	403220.538919	38.848320
2367.850890	403962.871425	38.853338
2370.096956	404701.485701	38.858356
2372.289032	405461.320984	38.863373
2374.916929	406206.191543	38.868391
2377.035001	406974.054052	38.873408
2379.406140	407731.618293	38.878426
2382.598585	408480.057910	38.883444
2384.589408	409252.589172	38.888461
2387.662340	410005.363469	38.893479
2390.014975	410762.060504	38.898496
2392.053848	411523.423336	38.903514
2394.771033	412279.966391	38.908532
2397.515957	413041.549006	38.913549
2399.805459	413795.915472	38.918567
2402.385488	414555.986926	38.923584
2404.919777	415309.661359	38.928602
2407.462780	416070.099813	38.933620
2409.869395	416834.995592	38.938637
2412.568889	417584.194946	38.943655
2414.795094	418339.350858	38.948672
2417.304462	419098.387997	38.953690
2419.750087	419851.360817	38.958708
2422.334851	420607.757195	38.963725
2424.840097	421366.625280	38.968743
2427.062737	422133.568654	38.973760
2429.529441	422878.901349	38.978778
2432.533357	423633.516057	38.983796
2434.345425	424388.911871	38.988813
2437.063904	425151.426068	38.993831
2439.385875	425899.551604	38.998848
2441.537986	426660.896686	39.003866
2444.189608	427424.869287	39.008884
2446.460142	428185.437788	39.013901
2449.010152	428945.530964	39.018919
2451.241717	429711.879181	39.023936
2454.089888	430474.506656	39.028954
2456.834746	431231.153230	39.033972
2458.883895	431998.064684	39.038989
2461.502907	432754.125998	39.044007
2464.130985	433518.209187	39.049024
2466.526171	434266.159612	39.054042
2469.371623	434995.689667	39.059060
2471.783686	435715.297647	39.064077
2474.439601	436429.579347	39.069095
2476.810912	437144.239853	39.074112
2479.217345	437864.489355	39.079130
2481.822325	438581.242003	39.084148
2484.077154	439301.217583	39.089165
2486.310376	440017.580882	39.094183
2488.912627	440733.657896	39.099200
2491.013917	441471.703536	39.104218
2493.421772	442198.441550	39.109236
2495.524067	442949.643342	39.114253
2498.166854	443687.272482	39.119271
2500.492392	444440.207683	39.124288
2502.981435	445197.137040	39.129306
2505.602584	445945.924116	39.134324
2507.895767	446711.989198	39.139341
2510.454769	447481.928708	39.144359
2512.918515	448248.011984	39.149376
2515.339130	449018.171888	39.154394
2517.970919	449797.170889	39.159412
2520.244869	450594.812528	39.164429
2522.568965	451369.302925	39.169447
2525.164230	452156.110399	39.174464
2527.497245	452953.804303	39.179482
2530.278233	453751.697123	39.184500
2532.873807	454559.956081	39.189517
2535.235158	455363.974526	39.194535
2537.942723	456165.224525	39.199552
2540.238510	456978.392975	39.204570
2543.050706	457788.005736	39.209588
2545.519768	458618.674591	39.214605
2548.210814	459427.786730	39.219623
2551.065021	460242.804670	39.224640
2553.556478	461065.836356	39.229658
2556.046836	461889.794696	39.234676
2558.402591	462716.369504	39.239693
2561.227336	463542.680771	39.244711
2563.878995	464385.563897	39.249728
2566.178467	465202.592222	39.254746
2569.387295	466041.420524	39.259764
2571.626828	466884.162772	39.264781
2574.444267	467716.464121	39.269799
2576.981686	468560.398059	39.274816
2579.594451	469392.256492	39.279834
2582.489258	470216.402621	39.284852
2584.947721	471062.159322	39.289869
2587.889467	471894.056411	39.294887
2590.445423	472722.444099	39.299904
2593.095708	473550.325128	39.304922
2595.979040	474380.151826	39.309940
2598.533207	475218.936936	39.314957
2601.242501	476048.667584	39.319975
2603.865923	476883.729257	39.324992
2606.483596	477717.541947	39.330010
2609.261711	478539.118714	39.335028
2611.937923	479378.654356	39.340045
2614.424696	480199.851056	39.345063
2616.931698	481037.924138	39.350080
2619.193507	481863.728466	39.355098
2621.824824	482704.380054	39.360116
2624.522196	483536.700922	39.365133
2627.150594	484367.681774	39.370151
2629.642593	485212.176712	39.375168
2632.485345	486055.765916	39.380186
2635.340207	486893.406597	39.385204
2637.835475	487719.254722	39.390221
2640.275772	488552.493160	39.395239
2643.079858	489354.741686	39.400256
2645.268319	490163.111493	39.405274
2648.157395	490964.716612	39.410292
2650.639811	491774.931133	39.415309
2653.057976	492576.135456	39.420327
2655.574342	493382.029725	39.425344
2658.308951	494200.767880	39.430362
2660.432291	495020.879496	39.435380
2662.825195	495846.053547	39.440397
2665.359816	496671.719029	39.445415
2667.899952	497505.465733	39.450432
2670.090734	498360.215019	39.455450
2672.993602	499201.031744	39.460468
2675.526751	500067.138874	39.465485
2678.212916	500929.443137	39.470503
2681.274231	501800.063706	39.475520
2683.750207	502674.618405	39.480538
2686.360925	503543.254307	39.485556
2688.858700	504423.007695	39.490573
2691.438479	505306.431751	39.495591
2694.075798	506200.135243	39.500608
2697.080789	507094.585995	39.505626
2699.754475	507991.209852	39.510644
2702.323439	508903.177710	39.515661
2705.025713	509795.057972	39.520679
2708.016623	510707.004692	39.525696
2710.365758	511622.029416	39.530714
2713.287369	512531.715329	39.535732
2715.799427	513462.735977	39.540749
2719.003735	514378.115227	39.545767
2721.776415	515293.008271	39.550784
2724.268724	516224.220978	39.555802
2727.091858	517147.765065	39.560820
2729.922209	518090.449986	39.565837
2732.600158	519012.596698	39.570855
2735.616560	519948.940205	39.575872
2738.071269	520882.749959	39.580890
2741.206720	521812.662707	39.585908
2744.026439	522751.335184	39.590925
2746.631801	523690.538952	39.595943
2749.529388	524629.736867	39.600960
2752.351600	525576.090251	39.605978
2755.409124	526514.841772	39.610996
2758.547582	527457.347924	39.616013
2761.286382	528391.451600	39.621031
2764.044563	529321.566079	39.626048
2766.978102	530274.147774	39.631066
2769.721294	531196.191996	39.636084
2772.379520	532133.092596	39.641101
2775.126065	533081.193772	39.646119
2778.311792	534005.152302	39.651136
2781.002909	534959.280730	39.656154
2783.868109	535894.546010	39.661172
2786.672500	536831.572248	39.666189
2789.455295	537777.900297	39.671207
2792.494867	538714.664045	39.676224
2794.958139	539654.832255	39.681242
2797.994364	540603.346050	39.686260
2801.028447	541545.156302	39.691277
2803.522018	542478.743231	39.696295
2806.394950	543414.066707	39.701312
2809.136281	544359.157157	39.706330
2811.937722	545292.556206	39.711348
2814.765853	546238.309660	39.716365
2817.713127	547179.905859	39.721383
2820.530977	548106.072923	39.726400
2823.220567	549053.466815	39.731418
2825.950174	549984.750926	39.736436
2828.821675	550890.711742	39.741453
2831.743836	551793.638183	39.746471
2834.470101	552683.870096	39.751488
2837.351486	553588.593951	39.756506
2840.172895	554487.135551	39.761524
2842.671730	555392.655882	39.766541
2845.528907	556305.945586	39.771559
2848.279179	557207.432444	39.776576
2850.642167	558135.250634	39.781594
2853.659031	559047.070181	39.786612
2856.214877	559975.280611	39.791629
2858.891990	560909.936304	39.796647
2861.881916	561852.310080	39.801664
2864.766919	562790.414396	39.806682
2867.503133	563736.361078	39.811700
2870.167830	564697.316906	39.816717
2872.988046	565658.427113	39.821735
2875.977835	566615.119765	39.826752
2878.570147	567593.547432	39.831770
2881.480202	568564.819625	39.836788
2884.507524	569547.996966	39.841805
2887.135149	570526.395853	39.846823
2890.222765	571517.543423	39.851840
2892.783833	572512.113314	39.856858
2895.913716	573502.697156	39.861876
2898.490135	574506.793253	39.866893
2901.290939	575516.743251	39.871911
2904.701211	576521.042437	39.876928
2907.695772	577529.844608	39.881946
2910.254134	578543.001289	39.886964
2913.367256	579557.338080	39.891981
2916.047333	580586.810417	39.896999
2919.384155	581609.016900	39.902016
2922.169920	582640.005115	39.907034
2925.134357	583668.770940	39.912052
2928.188398	584709.869920	39.917069
2931.108584	585745.035905	39.922087
2934.294094	586776.209551	39.927104
2937.282156	587825.423550	39.932122
2940.029742	588862.105139	39.937140
2943.003073	589905.927049	39.942157
2946.051064	590951.148894	39.947175
2949.386201	591991.170594	39.952192
2952.019878	593047.300590	39.957210
2955.079340	594095.099699	39.962228
2958.334075	595138.966184	39.967245
2961.056804	596192.896113	39.972263
2964.321036	597242.885390	39.977280
2967.090482	598297.970247	39.982298
2970.447391	599349.958043	39.987316
2973.334473	600411.241567	39.992333
2976.255599	601463.409615	39.997351
2979.158488	602511.980069	40.002368
2982.163890	603572.852729	40.007386
2985.176544	604625.116475	40.012404
2988.279043	605684.375539	40.017421
2990.955839	606747.509698	40.022439
2994.112310	607806.862091	40.027456
2997.137196	608875.593738	40.032474
3000.228694	609926.301593	40.037492
3003.044335	610984.660743	40.042509
3006.012839	612063.153612	40.047527
3009.329110	613118.626858	40.052544
3012.376209	614188.497932	40.057562
3015.288638	615251.286799	40.062580
3018.801122	616310.524259	40.067597
3021.407263	617378.258925	40.072615
3024.991518	618407.583446	40.077632
3027.780982	619435.792394	40.082650
3030.712171	620446.486558	40.087668
3033.805137	621465.156789	40.092685
3036.300471	622468.387596	40.097703
3039.597426	623484.285449	40.102720
3042.434951	624492.768372	40.107738
3045.466008	625510.167630	40.112756
3048.368261	626532.986650	40.117773
3051.415802	627580.509477	40.122791
3054.452169	628605.605124	40.127808
3057.428359	629650.038899	40.132826
3060.103840	630687.977373	40.137844
3063.258867	631738.067771	40.142861
3065.986313	632788.573164	40.147879
3069.096132	633839.808880	40.152896
3071.802580	634909.324711	40.157914
3074.881273	635977.072280	40.162932
3077.861222	637066.385632	40.167949
3080.722926	638156.452240	40.172967
3083.657961	639246.940546	40.177984
3086.892623	640354.126808	40.183002
3089.754552	641455.368658	40.188020
3093.295127	642561.268263	40.193037
3095.580524	643675.134919	40.198055
3099.149704	644794.303049	40.203072
3102.186235	645936.172811	40.208090
3105.060912	647057.448886	40.213108
3108.286822	648197.386116	40.218125
3111.384633	649340.803902	40.223143
3114.525218	650482.887804	40.228160
3117.616752	651637.506956	40.233178
3120.741322	652795.474570	40.238196
3124.051596	653951.482643	40.243213
3127.140793	655117.953054	40.248231
3130.600941	656274.112498	40.253248
3133.703867	657433.830402	40.258266
3136.544592	658609.091007	40.263284
3139.774448	659767.963067	40.268301
3142.926567	660956.831047	40.273319
3146.463583	662130.406065	40.278336
3149.862027	663305.752774	40.283354
3152.863559	664482.813109	40.288372
3156.260191	665650.109503	40.293389
3159.341506	666833.436632	40.298407
3162.585441	668011.167327	40.303424
3165.949092	669194.850944	40.308442
3169.238418	670368.252375	40.313460
3172.867189	671549.657877	40.318477
3176.123489	672721.677838	40.323495
3179.270934	673884.520457	40.328512
3182.552281	675064.993902	40.333530
3185.987741	676241.266307	40.338548
3189.590975	677398.177775	40.343565
3192.567584	678564.837999	40.348583
3195.301935	679728.707749	40.353600
3198.792225	680899.460132	40.358618
3201.939408	682074.590673	40.363636
3205.464091	683237.388913	40.368653
3208.250378	684412.725500	40.373671
3211.734886	685569.025090	40.378688
3214.984053	686738.373453	40.383706
3218.364301	687897.818905	40.388724
3221.467251	689071.109148	40.393741
3224.925323	690235.800179	40.398759
3228.045239	691398.906923	40.403776
3231.494905	692561.311819	40.408794
3234.506340	693723.835792	40.413812
3237.777889	694858.832402	40.418829
3241.108467	695989.061204	40.423847
3243.967642	697094.178861	40.428864
3247.367942	698209.085178	40.433882
3250.385999	699323.764264	40.438900
3253.497049	700429.362920	40.443917
3256.686015	701557.510723	40.448935
3260.124684	702679.821321	40.453952
3263.019396	703816.942933	40.458970
3265.963309	704939.785976	40.463988
3269.217675	706068.178729	40.469005
3272.313280	707213.143137	40.474023
3275.617350	708353.958282	40.479040
3278.845463	709513.056079	40.484058
3281.767825	710680.811091	40.489076
3285.338012	711837.407400	40.494093
3288.437923	713026.198537	40.499111
3291.966416	714189.311993	40.504128
3294.969706	715371.849836	40.509146
3297.983680	716553.922900	40.514164
3301.389270	717732.202835	40.519181
3304.656574	718936.012787	40.524199
3308.278502	720135.188723	40.529216
3311.262211	721335.286008	40.534234
3314.551894	722554.690020	40.539252
3317.819737	723771.198762	40.544269
3321.077244	724999.590730	40.549287
3324.250364	726232.656502	40.554304
3327.888436	727456.664205	40.559322
3331.074403	728690.691721	40.564340
3334.838638	729928.487889	40.569357
3337.991630	731178.248041	40.574375
3341.238164	732417.527802	40.579392
3345.063597	733663.582992	40.584410
3347.851640	734904.383042	40.589428
3351.528379	736154.421180	40.594445
3354.848890	737429.542957	40.599463
3358.437670	738677.769544	40.604480
3362.275465	739933.505458	40.609498
3365.320650	741189.469149	40.614516
3368.581097	742447.762728	40.619533
3372.039512	743704.343423	40.624551
3375.353633	744973.024606	40.629568
3379.229493	746238.548504	40.634586
3382.561326	747507.358200	40.639604
3386.256224	748770.726689	40.644621
3389.418780	750043.389034	40.649639
3392.762784	751300.342436	40.654656
3396.660543	752577.393355	40.659674
3399.806821	753847.116371	40.664692
3403.254179	755102.496294	40.669709
3406.730768	756383.710759	40.674727
3410.261247	757646.241302	40.679744
3413.618062	758914.546424	40.684762
3417.154810	760188.367487	40.689780
3420.605372	761441.864685	40.694797
3424.129390	762718.656085	40.699815
3427.307051	763996.222340	40.704832
3431.279376	765265.030779	40.709850
3434.262101	766527.296710	40.714868
3437.816180	767793.285978	40.719885
3441.132808	769063.325859	40.724903
3444.451182	770332.803879	40.729920
3448.091465	771602.747875	40.734938
3451.556875	772882.523677	40.739956
3455.342235	774143.948506	40.744973
3458.457795	775426.580075	40.749991
3461.726297	776686.325838	40.755008
3465.295408	777926.744849	40.760013
3468.494087	779154.007831	40.765018
3471.876482	780304.474821	40.770023
3475.234489	781397.992427	40.775028
3478.192717	782428.696256	40.780032
3481.610051	783395.340252	40.785037
3484.383203	784289.722840	40.790042
3487.325353	785114.244485	40.795047
3489.903300	785879.439718	40.800052
3492.362941	786575.799264	40.805056
3494.761110	787204.710137	40.810061
3497.022917	787779.718916	40.815066
3499.910229	788284.445373	40.820071
3501.678944	788733.836747	40.825076
3503.459420	789114.498268	40.830080
3505.447168	789447.931754	40.835085
3507.167996	789744.983014	40.840090
3508.936091	789971.750574	40.845095
3510.269171	790163.402542	40.850100
3511.560775	790310.148577	40.855104
3513.427997	790411.938937	40.860109
3514.049962	790467.257687	40.865114
3515.705578	790486.392085	40.870119
3516.653475	790486.137685	40.875124
3517.418798	790442.480607	40.880128
3518.542308	790365.894505	40.885133
3519.371321	790259.384726	40.890138
3520.100388	790128.617458	40.895143
3520.874533	789970.373657	40.900148
3521.283073	789799.804126	40.905152
3522.176084	789601.240302	40.910157
3522.751096	789384.836535	40.915162
3523.263296	789138.853533	40.920167
3523.732981	788888.052996	40.925172
3524.280164	788624.010884	40.930176
3524.700121	788343.073449	40.935181
3524.872039	788040.835199	40.940186
3525.514692	787714.766593	40.945191
3525.607658	787397.277146	40.950196
3525.644011	787072.163762	40.955200
3525.868495	786724.244448	40.960205
3526.163130	786378.459657	40.965210
3526.409856	786019.047920	40.970215
3526.175346	785655.616666	40.975220
3526.209283	785282.239960	40.980224
3526.791925	784905.360597	40.985229
3526.842362	784525.598705	40.990234
3526.497039	784128.572028	40.995239
3526.935032	783748.459232	41.000244
3526.831871	783350.611924	41.005248
3527.032662	782951.069433	41.010253
3526.440682	782548.290670	41.015258
3526.874358	782142.713329	41.020263
3526.892715	781741.018574	41.025268
3526.576461	781328.041737	41.030272
3527.127498	780927.197795	41.035277
3526.790434	780516.687052	41.040282
3526.868195	780100.426266	41.045287
3526.900723	779678.244248	41.050292
3526.517151	779266.686115	41.055296
3526.576727	778845.976625	41.060301
3526.426551	778435.120232	41.065306
3526.191440	778016.773540	41.070311
3526.110181	777605.022154	41.075316
3526.290310	777183.556682	41.080320
3526.002775	776777.699255	41.085325
3525.699077	776365.963687	41.090330
3526.002385	775943.027801	41.095335
3525.779494	775529.360935	41.100340
3525.647191	775117.231317	41.105344
3525.571785	774696.944539	41.110349
3525.469955	774289.588806	41.115354
3525.449055	773874.564073	41.120359
3525.490843	773471.669821	41.125364
3525.339383	773052.975792	41.130368
3525.041745	772639.256619	41.135373
3524.770921	772244.670482	41.140378
3524.836441	771814.639789	41.145383
3524.561646	771427.054572	41.150388
3524.260373	771016.890252	41.155392
3524.502898	770617.797201	41.160397
3523.841660	770223.364334	41.165402
3524.166078	769824.609145	41.170407
3523.855624	769432.934152	41.175412
3523.866136	769033.350423	41.180416
3523.640189	768629.890983	41.185421
3523.284938	768247.967582	41.190426
3523.271240	767852.414766	41.195431
3523.134181	767479.188737	41.200436
3522.855334	767086.004690	41.205440
3522.952432	766699.244650	41.210445
3522.218786	766332.911237	41.215450
3522.300712	765951.833235	41.220455
3522.234317	765584.860195	41.225460
3522.191615	765222.154593	41.230464
3521.787047	764851.947319	41.235469
3521.668766	764492.078504	41.240474
3521.718076	764118.949685	41.245479
3521.394060	763761.890402	41.250484
3520.989392	763414.049295	41.255488
3521.168857	763051.399333	41.260493
3520.765598	762697.508134	41.265498
3520.840983	762345.938194	41.270503
3520.666511	762008.844961	41.275508
3520.397801	761656.165082	41.280512
3520.295995	761299.100293	41.285517
3520.105422	760978.242092	41.290522
3520.238875	760617.061178	41.295527
3520.050004	760293.953661	41.300532
3519.628324	759958.191006	41.305536
3519.353419	759612.620035	41.310541
3519.562629	759299.272411	41.315546
3519.291368	758966.796279	41.320551
3519.172355	758651.156812	41.325556
3518.552974	758328.579261	41.330560
3518.749632	758006.495111	41.335565
3518.206082	757695.722222	41.340570
3518.299853	757379.649451	41.345575
3518.211522	757066.505587	41.350580
3518.006812	756761.857642	41.355584
3517.947582	756455.890198	41.360589
3517.466339	756159.457542	41.365594
3517.581783	755855.609198	41.370599
3516.959399	755564.705488	41.375604
3517.056846	755270.166996	41.380608
3516.444444	754982.102818	41.385613
3516.219800	754708.972831	41.390618
3516.039821	754427.926044	41.395623
3516.529973	754151.597294	41.400628
3516.202778	753884.626720	41.405632
3516.336240	753608.337195	41.410637
3515.965386	753336.663815	41.415642
3516.002714	753060.074147	41.420647
3515.680987	752797.558674	41.425652
3515.566491	752526.357662	41.430656
3515.524693	752266.148453	41.435661
3515.253983	751999.152528	41.440666
3515.047656	751730.605646	41.445671
3515.094809	751485.172575	41.450676
3514.932199	751232.999336	41.455680
3514.853036	750980.754722	41.460685
3514.916558	750734.356601	41.465690
3514.843114	750461.693182	41.470695
3514.414855	750229.339807	41.475700
3514.333658	749984.423664	41.480704
3514.906642	749733.760027	41.485709
3514.597720	749492.669923	41.490714
3514.220009	749240.220197	41.495719
3514.076420	748991.231652	41.500724
3513.972276	748755.618607	41.505728
3514.101013	748510.324903	41.510733
3513.444924	748285.560153	41.515738
3513.295037	748055.912350	41.520743
3513.482492	747831.687296	41.525748
3513.122141	747602.900873	41.530752
3513.340986	747369.317564	41.535757
3512.990880	747160.926202	41.540762
3513.227309	746927.475025	41.545767
3513.040271	746710.692605	41.550772
3512.733337	746485.867833	41.555776
3512.848597	746273.076216	41.560781
3512.679929	746053.603575	41.565786
3512.672493	745829.501405	41.570791
3512.328481	745612.862686	41.575796
3512.471765	745408.544792	41.580800
3512.166445	745204.789805	41.585805
3511.990738	744996.312003	41.590810
3511.992170	744793.385579	41.595815
3511.711646	744603.650283	41.600820
3511.553545	744408.007230	41.605824
3511.829383	744205.613641	41.610829
3511.850845	744017.396446	41.615834
3511.747606	743803.931091	41.620839
3511.361204	743619.529072	41.625844
3511.283257	743431.413114	41.630848
3511.455284	743232.522050	41.635853
3510.862850	743044.234388	41.640858
3511.422786	742855.109541	41.645863
3511.280262	742668.518851	41.650868
3510.976789	742482.543653	41.655872
3511.087740	742299.462799	41.660877
3510.781337	742119.561901	41.665882
3510.846725	741922.583972	41.670887
3510.633947	741744.488847	41.675892
3510.415132	741569.011806	41.680896
3510.369759	741393.255012	41.685901
3510.251455	741237.882585	41.690906
3510.607819	741048.649120	41.695911
3510.297972	740888.009370	41.700916
3510.090436	740711.769569	41.705920
3510.552000	740539.125193	41.710925
3510.033457	740370.150372	41.715930
3510.002091	740195.700169	41.720935
3510.002389	740035.635059	41.725940
3509.733741	739880.161846	41.730944
3510.011273	739706.540368	41.735949
3509.565164	739539.811375	41.740954
3509.695164	739371.945116	41.745959
3509.560635	739225.489718	41.750964
3509.343696	739059.257041	41.755968
3509.485753	738900.877172	41.760973
3508.894010	738754.340014	41.765978
3509.310913	738600.707702	41.770983
3508.989323	738448.727810	41.775988
3509.014710	738293.422482	41.780992
3509.083573	738143.747246	41.785997
3508.855325	738003.469315	41.791002
3508.721423	737843.332713	41.796007
3508.754489	737710.675662	41.801012
3508.430337	737569.762677	41.806016
3508.894639	737424.956766	41.811021
3508.545565	737278.055582	41.816026
3508.321482	737135.386587	41.821031
3508.199247	736993.489994	41.826036
3508.155899	736867.561249	41.831040
3508.275238	736737.397502	41.836045
3507.811762	736607.773038	41.841050
3508.213430	736465.137431	41.846055
3508.021100	736340.313636	41.851060
3507.774838	736199.908016	41.856064
3508.055587	736073.319511	41.861069
3507.806188	735955.625528	41.866074
3507.972623	735822.667725	41.871079
3508.009415	735687.304002	41.876084
3507.922378	735562.599210	41.881088
3507.734572	735433.207257	41.886093
3507.728928	735312.840546	41.891098
3507.854823	735193.638221	41.896103
3507.688220	735063.791367	41.901108
3507.266761	734939.725937	41.906112
3507.551930	734811.334936	41.911117
3507.443951	734695.183049	41.916122
3507.359295	734573.729333	41.921127
3507.410565	734457.894265	41.926132
3507.133807	734342.804572	41.931136
3507.330662	734216.646110	41.936141
3506.926748	734110.731619	41.941146
3507.206978	733988.515927	41.946151
3507.248204	733870.594982	41.951156
3506.737627	733758.802627	41.956160
3507.207513	733650.906488	41.961165
3507.166023	733553.835646	41.966170
3507.123835	733432.357706	41.971175
3506.767554	733315.979296	41.976180
3506.837743	733211.311513	41.981184
3506.863392	733098.381998	41.986189
3506.723760	732990.032869	41.991194
3506.769529	732883.186503	41.996199
3506.527495	732774.257245	42.001204
3506.524131	732677.862707	42.006208
3506.687748	732565.497122	42.011213
3506.445941	732464.386309	42.016218
3506.454434	732354.271348	42.021223
3506.484794	732251.182059	42.026228
3506.038758	732160.449194	42.031232
3506.092731	732050.966277	42.036237
3505.944878	731969.441192	42.041242
3506.138974	731864.438454	42.046247
3506.140795	731768.675911	42.051252
3505.889531	731672.755871	42.056256
3506.386484	731578.692075	42.061261
3506.138429	731490.642483	42.066266
3505.602583	731387.437412	42.071271
3505.850494	731301.779934	42.076276
3505.932091	731202.679826	42.081280
3506.047205	731111.892256	42.086285
3505.805647	731039.138179	42.091290
3505.724437	730950.015301	42.096295
3505.653976	730861.582965	42.101300
3505.332158	730768.090362	42.106304
3506.063320	730676.007890	42.111309
3505.693248	730593.267514	42.116314
3505.532647	730501.676659	42.121319
3505.460941	730414.477734	42.126324
3505.551739	730334.085438	42.131328
3505.377625	730247.297784	42.136333
3505.324410	730174.851594	42.141338
3505.289548	730083.086722	42.146343
3505.131255	730002.038823	42.151348
3505.237905	729928.969784	42.156352
3505.026967	729846.393680	42.161357
3505.050017	729764.174403	42.166362
3505.242254	729685.492446	42.171367
3504.983405	729618.374687	42.176372
3505.064372	729531.983121	42.181376
3505.108533	729462.832988	42.186381
3505.040466	729406.033702	42.191386
3505.062668	729319.550503	42.196391
3505.259214	729252.949059	42.201396
3504.821798	729167.778248	42.206400
3504.956965	729078.599186	42.211405
3505.076208	729009.630961	42.216410
3504.839208	728933.241412	42.221415
3504.713243	728858.715111	42.226420
3504.571642	728794.493695	42.231424
3505.103675	728718.767958	42.236429
3504.832231	728662.244665	42.241434
3504.661323	728583.661435	42.246439
3504.845138	728516.758864	42.251444
3504.738256	728451.191570	42.256448
3504.835277	728384.549894	42.261453
3504.692777	728314.182368	42.266458
3504.677632	728243.149271	42.271463
3504.834760	728169.015853	42.276468
3504.368627	728096.668744	42.281472
3504.621595	728028.809561	42.286477
3504.346145	727974.115071	42.291482
3504.636494	727904.465308	42.296487
3504.819130	727845.879978	42.301492
3504.722274	727774.261794	42.306496
3504.725717	727703.468638	42.311501
3504.500876	727644.899467	42.316506
3504.619110	727573.541326	42.321511
3504.440864	727507.383719	42.326516
3504.521643	727440.538853	42.331520
3504.462911	727384.615702	42.336525
3504.318075	727311.911444	42.341530
3504.154738	727247.978696	42.346535
3504.208260	727187.824551	42.351540
3504.043790	727134.097016	42.356544
3504.362707	727070.132960	42.361549
3504.415602	727017.458812	42.366554
3503.939260	726951.444913	42.371559
3503.993504	726883.014432	42.376564
3504.181255	726832.348225	42.381568
3504.074007	726769.294312	42.386573
3503.794481	726723.064456	42.391578
3504.091457	726659.695365	42.396583
3504.042903	726610.553117	42.401588
3503.892136	726550.427952	42.406592
3504.124915	726498.464034	42.411597
3503.943752	726431.505448	42.416602
3504.091971	726379.356518	42.421607
3503.951475	726327.502571	42.426612
3503.805271	726282.338325	42.431616
3503.816582	726215.296710	42.436621
3504.093334	726171.796387	42.441626
3503.974513	726113.545632	42.446631
3503.996856	726067.658735	42.451636
3504.094239	726021.362815	42.456640
3504.195054	725949.299690	42.461645
3503.978978	725903.897119	42.466650
3503.841391	725834.250716	42.471655
3503.912561	725794.696838	42.476660
3503.975207	725734.431421	42.481664
3504.143058	725677.022270	42.486669
3503.714180	725623.328394	42.491674
3503.950775	725565.907139	42.496679
3504.100489	725517.369865	42.501684
3503.943239	725461.846253	42.506688
3504.227883	725394.306913	42.511693
3504.003050	725351.727316	42.516698
3503.427451	725288.540973	42.521703
3503.629726	725230.231042	42.526708
3503.916637	725189.944933	42.531712
3503.977071	725124.868537	42.536717
3504.114892	725079.006646	42.541722
3503.815537	725025.931750	42.546727
3503.736697	724975.991804	42.551732
3503.858835	724922.549451	42.556736
3504.051867	724857.349976	42.561741
3503.973485	724812.265584	42.566746
3503.552659	724757.474450	42.571751
3503.975483	724702.246593	42.576756
3503.252425	724654.194941	42.581760
3503.771542	724595.084926	42.586765
3503.229542	724562.613965	42.591770
3503.314985	724517.104489	42.596775
3503.726527	724486.805406	42.601780
3503.179687	724439.466857	42.606784
3503.605118	724393.999800	42.611789
3503.423851	724352.993778	42.616794
3503.618368	724307.415611	42.621799
3503.325148	724255.821554	42.626804
3503.192547	724207.025704	42.631808
3503.739007	724158.068114	42.636813
3503.409158	724118.225321	42.641818
3503.545029	724072.705082	42.646823
3503.409234	724030.054409	42.651828
3503.362317	723990.511316	42.656832
3503.652370	723932.078609	42.661837
3503.278344	723897.793078	42.666842
3503.293450	723844.262240	42.671847
3503.481578	723812.609720	42.676852
3503.109167	723767.716748	42.681856
3503.485175	723730.531356	42.686861
3503.344280	723693.976175	42.691866
3503.504813	723646.020863	42.696871
3503.306786	723595.150455	42.701876
3503.187151	723565.232906	42.706880
3503.141265	723518.252601	42.711885
3503.296281	723479.962490	42.716890
3503.164960	723438.695860	42.721895
3503.067211	723397.820022	42.726900
3503.399015	723366.885612	42.731904
3503.497979	723322.110811	42.736909
3503.494800	723275.716889	42.741914
3503.304013	723231.831978	42.746919
3503.477514	723186.102382	42.751924
3503.482148	723138.318513	42.756928
3503.533016	723085.123835	42.761933
3503.080473	723047.377940	42.766938
3503.363740	722997.267205	42.771943
3503.608760	722956.134428	42.776948
3503.486157	722910.799081	42.781952
3503.625772	722875.928976	42.786957
3503.357184	722838.597939	42.791962
3503.173256	722799.666552	42.796967
3503.053382	722764.888304	42.801972
3503.059039	722710.657697	42.806977
3503.286827	722674.086824	42.811981
3502.930149	722636.372823	42.816986
3503.129297	722598.467924	42.821991
3502.923457	722567.272119	42.826996
3502.980581	722520.269168	42.832001
3503.556935	722488.696326	42.837005
3503.375493	722451.547468	42.842010
3503.220343	722399.373762	42.847015
3503.117029	722366.276563	42.852020
3503.256485	722324.464030	42.857025
3502.851540	722271.735807	42.862029
3502.842046	722242.092755	42.867034
3503.102830	722206.456269	42.872039
3502.909527	722171.935494	42.877044
3503.077566	722143.948339	42.882049
3503.197175	722099.560109	42.887053
3502.844077	722067.196906	42.892058
3503.255356	722035.005075	42.897063
3503.191152	721992.926980	42.902068
3502.946735	721965.007181	42.907073
3503.313412	721916.165106	42.912077
3502.801264	721885.810402	42.917082
3502.948067	721840.375223	42.922087
3503.040994	721813.886595	42.927092
3502.976407	721771.410833	42.932097
3503.070443	721737.039203	42.937101
3503.076146	721702.979444	42.942106
3503.330586	721661.937844	42.947111
3503.104648	721618.099739	42.952116
3503.049535	721593.915335	42.957121
3503.082728	721543.341243	42.962125
3502.885210	721521.411068	42.967130
3503.014022	721477.117145	42.972135
3503.072917	721444.733201	42.977140
3503.283315	721401.863192	42.982145
3503.032529	721367.596427	42.987149
3502.890279	721330.485660	42.992154
3503.087032	721285.435842	42.997159
3503.152343	721251.166091	43.002164
3502.903122	721219.426985	43.007169
3503.102020	721180.920699	43.012173
3503.130893	721155.828749	43.017178
3503.038364	721109.982792	43.022183
3503.194230	721079.217580	43.027188
3503.162738	721037.525888	43.032193
3503.110249	721006.100612	43.037197
3503.147997	720964.297983	43.042202
3503.279072	720918.860353	43.047207
3503.200685	720882.927006	43.052212
3503.099194	720843.477029	43.057217
3503.283908	720797.732410	43.062221
3503.278744	720766.100102	43.067226
3503.165906	720721.643641	43.072231
3503.333598	720691.569196	43.077236
3503.044443	720653.735874	43.082241
3503.082141	720602.213240	43.087245
3502.887017	720575.024381	43.092250
3503.232021	720532.573957	43.097255
3503.131573	720490.890884	43.102260
3502.903495	720469.557966	43.107265
3502.980474	720417.283959	43.112269
3502.883416	720395.929263	43.117274
3502.766442	720354.149060	43.122279
3502.709024	720323.664119	43.127284
3502.799422	720295.782700	43.132289
3502.773652	720263.705613	43.137293
3502.740302	720217.646641	43.142298
3503.005897	720197.570482	43.147303
3503.103012	720168.001628	43.152308
3503.041464	720131.368061	43.157313
3502.792140	720089.013305	43.162317
3502.869206	720060.439092	43.167322
3503.037070	720021.287934	43.172327
3502.954759	719991.301740	43.177332
3502.790951	719958.452837	43.182337
3503.064822	719917.349841	43.187341
3503.083588	719888.635884	43.192346
3502.819483	719848.761696	43.197351
3503.048911	719811.334966	43.202356
3503.065039	719778.455704	43.207361
3503.173713	719749.329751	43.212365
3503.004867	719706.811025	43.217370
3502.883866	719668.846336	43.222375
3503.071600	719630.929782	43.227380
3503.059925	719601.327254	43.232385
3502.967310	719564.101245	43.237389
3502.716376	719540.835735	43.242394
3502.849239	719506.398900	43.247399
3502.840355	719467.670980	43.252404
3502.747061	719442.246865	43.257409
3503.258106	719408.739109	43.262413
3502.929638	719374.972825	43.267418
3503.067947	719341.427036	43.272423
3502.903546	719304.905962	43.277428
3502.760223	719269.422662	43.282433
3502.725129	719234.169334	43.287437
3502.869763	719197.894417	43.292442
3502.921152	719163.172043	43.297447
3502.853805	719132.386829	43.302452
3502.902057	719103.070208	43.307457
3502.987112	719074.144156	43.312461
3502.982875	719037.843482	43.317466
3502.969928	718996.783212	43.322471
3502.931694	718972.489219	43.327476
3502.844542	718934.168459	43.332481
3503.101315	718884.037295	43.337485
3502.551185	718863.249253	43.342490
3502.822767	718825.612785	43.347495
3502.717879	718795.229260	43.352500
3503.049910	718764.922415	43.357505
3502.938279	718733.002366	43.362509
3502.843653	718700.781828	43.367514
3503.212408	718675.229649	43.372519
3503.315514	718638.215229	43.377524
3503.057432	718592.481877	43.382529
3503.187210	718549.660072	43.387533
3503.014770	718522.708747	43.392538
3503.046767	718480.150674	43.397543
3503.129581	718456.579167	43.402548
3502.972928	718408.645886	43.407553
3503.087914	718378.770172	43.412557
3503.024953	718342.972116	43.417562
3502.752791	718298.330591	43.422567
3502.862837	718266.471426	43.427572
3502.927495	718240.372866	43.432577
3502.858794	718197.929142	43.437581
3502.751434	718167.047767	43.442586
3503.109917	718134.204814	43.447591
3503.012723	718099.998480	43.452596
3502.696324	718061.661893	43.457601
3503.068126	718029.857894	43.462605
3502.815911	718013.432880	43.467610
3502.942252	717969.616706	43.472615
3502.929544	717946.803481	43.477620
3502.574539	717912.440464	43.482625
3502.780049	717872.727444	43.487629
3502.760718	717850.807833	43.492634
3502.668365	717816.450743	43.497639
3502.593395	717785.463424	43.502644
3502.652400	717759.116296	43.507649
3502.789088	717731.615486	43.512653
3502.368667	717704.305583	43.517658
3502.627875	717667.459548	43.522663
3503.009202	717644.729375	43.527668
3502.776023	717617.090731	43.532673
3502.676647	717577.376948	43.537677
3502.800392	717554.143362	43.542682
3502.818895	717515.054673	43.547687
3502.881765	717492.971776	43.552692
3503.084277	717461.391922	43.557697
3502.884230	717417.180224	43.562701
3502.776095	717386.494504	43.567706
3502.960894	717349.758539	43.572711
3502.855621	717314.409474	43.577716
3502.720059	717294.590859	43.582721
3502.840747	717240.404867	43.587725
3503.098692	717223.100592	43.592730
3502.410963	717187.499743	43.597735
3502.940303	717155.319250	43.602740
3502.531124	717138.075120	43.607745
3502.694061	717111.609625	43.612749
3502.435100	717082.882185	43.617754
3502.357543	717039.491575	43.622759
3502.833551	717022.498186	43.627764
3502.555411	716993.773601	43.632769
3502.300725	716962.812851	43.637773
3502.705030	716940.523427	43.642778
3502.517917	716912.626844	43.647783
3502.686905	716888.094234	43.652788
3502.704472	716857.931521	43.657793
3502.807840	716829.986799	43.662797
3502.676906	716798.260971	43.667802
3502.582452	716764.147940	43.672807
3503.040025	716730.687899	43.677812
3502.419109	716704.201459	43.682817
3502.706487	716672.009379	43.687821
3502.655445	716641.658769	43.692826
3502.543546	716616.675584	43.697831
3502.700950	716582.272282	43.702836
3502.654775	716561.197036	43.707841
3502.455654	716516.236330	43.712845
3502.386660	716514.065024	43.717850
3502.192699	716475.651392	43.722855
3502.543007	716450.293910	43.727860
3502.433547	716427.492492	43.732865
3502.675031	716399.870836	43.737869
3502.186563	716367.606997	43.742874
3502.226802	716344.879904	43.747879
3502.610318	716328.297221	43.752884
3502.310522	716302.351896	43.757889
3502.588774	716279.089323	43.762893
3502.402034	716262.054778	43.767898
3502.562478	716232.511189	43.772903
3502.564813	716202.249413	43.777908
3502.540720	716179.383646	43.782913
3502.726823	716145.569137	43.787917
3502.490694	716119.463928	43.792922
3502.617163	716096.672347	43.797927
3503.075310	716070.502198	43.802932
3502.437228	716044.562207	43.807937
3502.510859	716000.297945	43.812941
3502.623981	715987.281468	43.817946
3502.861833	715947.206740	43.822951
3502.730959	715916.370558	43.827956
3502.704485	715902.335126	43.832961
3502.689299	715859.771526	43.837965
3502.490992	715841.001647	43.842970
3502.586306	715805.017839	43.847975
3502.550113	715786.121903	43.852980
3502.391169	715760.598198	43.857985
3502.957941	715724.585975	43.862989
3502.699997	715702.154337	43.867994
3502.574853	715672.755064	43.872999
3502.334626	715639.802564	43.878004
3502.429638	715621.579211	43.883009
3502.564002	715589.110528	43.888013
3502.428159	715558.621141	43.893018
3502.472362	715529.888043	43.898023
3502.603300	715499.999454	43.903028
3502.212170	715477.936455	43.908033
3502.702888	715451.709407	43.913037
3502.556204	715441.562860	43.918042
3502.381081	715411.823615	43.923047
3502.510967	715378.957950	43.928052
3502.414653	715360.070963	43.933057
3502.727462	715323.950035	43.938061
3502.751031	715305.588928	43.943066
3502.621279	715282.192375	43.948071
3502.685896	715250.279637	43.953076
3502.680205	715221.404865	43.958081
3502.684461	715182.357285	43.963085
3502.666590	715164.101928	43.968090
3502.718160	715125.840131	43.973095
3502.884202	715093.364318	43.978100
3502.459464	715068.031154	43.983105
3502.763318	715033.398928	43.988109
3502.586801	715015.566317	43.993114
3502.864567	714968.881431	43.998119
3503.016351	714954.418117	44.003124
3502.289717	714927.496933	44.008129
3502.999078	714885.354805	44.013133
3502.800629	714863.208826	44.018138
3503.069987	714828.283742	44.023143
3502.924881	714793.873361	44.028148
3502.675489	714766.972261	44.033153
3502.996200	714728.019286	44.038157
3503.007931	714696.907051	44.043162
3502.908244	714670.725245	44.048167
3502.986105	714638.659156	44.053172
3502.764065	714609.817938	44.058177
3503.006264	714575.888652	44.063181
3502.589844	714535.666928	44.068186
3502.943979	714507.772418	44.073191
3502.862474	714471.018148	44.078196
3502.489562	714444.533325	44.083201
3503.032300	714408.370595	44.088205
3502.651497	714379.802846	44.093210
3502.519627	714346.231993	44.098215
3503.059250	714322.623242	44.103220
3502.828414	714294.377834	44.108225
3502.782343	714250.620310	44.113229
3502.583000	714238.645030	44.118234
3502.717896	714193.616879	44.123239
3502.559561	714175.332905	44.128244
3502.750965	714140.665928	44.133249
3502.827911	714109.987375	44.138253
3502.629500	714073.746850	44.143258
3503.008074	714056.813177	44.148263
3502.925647	714012.316085	44.153268
3502.350759	713992.165097	44.158273
3502.611409	713956.394270	44.163277
3502.541668	713931.197679	44.168282
3503.040801	713893.849000	44.173287
3502.784082	713874.786625	44.178292
3502.866893	713843.709157	44.183297
3502.947621	713815.460433	44.188301
3502.650344	713790.598652	44.193306
3502.944430	713750.851592	44.198311
3502.556328	713717.022717	44.203316
3502.386468	713695.960680	44.208321
3502.498305	713646.368028	44.213325
3502.691316	713642.564838	44.218330
3502.431313	713608.565549	44.223335
3502.634216	713589.774167	44.228340
3502.536961	713554.358361	44.233345
3502.544169	713529.445641	44.238349
3502.622743	713494.993108	44.243354
3502.491887	713473.924092	44.248359
3502.551726	713443.047438	44.253364
3502.499146	713418.293117	44.258369
3502.589981	713391.381196	44.263373
3502.564584	713372.775827	44.268378
3502.427667	713337.713028	44.273383
3502.671370	713309.336509	44.278388
3502.583317	713288.706612	44.283393
3502.285431	713253.669988	44.288397
3502.848172	713231.592808	44.293402
3502.418514	713195.436247	44.298407
3502.642442	713177.434513	44.303412
3502.795536	713152.496646	44.308417
3502.698115	713112.761474	44.313421
3502.528863	713086.536593	44.318426
3502.612717	713065.629691	44.323431
3502.745082	713027.047313	44.328436
3502.506866	713016.515906	44.333441
3502.827538	712991.004046	44.338445
3502.318028	712960.269072	44.343450
3502.561907	712926.729924	44.348455
3502.967861	712900.955601	44.353460
3502.683190	712872.664681	44.358465
3502.959428	712837.432477	44.363469
3502.548032	712815.068068	44.368474
3502.814150	712785.048346	44.373479
3502.926648	712751.430895	44.378484
3502.758837	712723.020961	44.383489
3502.830339	712695.365574	44.388493
3502.657380	712659.412572	44.393498
3502.599623	712637.932391	44.398503
3503.152765	712604.936572	44.403508
3502.524593	712574.765681	44.408513
3502.609117	712544.030574	44.413517
3502.768235	712511.595622	44.418522
3502.780054	712478.390723	44.423527
3502.685728	712446.046913	44.428532
3502.538172	712421.553484	44.433537
3502.954424	712383.765134	44.438541
3502.686049	712357.554328	44.443546
3502.433887	712323.101897	44.448551
3502.711010	712301.218261	44.453556
3502.513775	712276.583703	44.458561
3502.635914	712233.582148	44.463565
3502.922868	712207.577169	44.468570
3502.390948	712189.251192	44.473575
3502.641978	712158.586519	44.478580
3502.575652	712126.584306	44.483585
3502.492685	712098.902794	44.488589
3502.526706	712074.825143	44.493594
3502.252643	712052.336822	44.498599
3502.681995	712025.712223	44.503604
3502.636834	712010.283664	44.508609
3502.787958	711970.700721	44.513613
3502.506989	711938.435362	44.518618
3502.545278	711906.911423	44.523623
3502.614210	711887.393835	44.528628
3502.355789	711872.546143	44.533633
3502.951791	711834.676102	44.538637
3502.911567	711801.973479	44.543642
3502.639007	711770.351348	44.548647
3502.894953	711740.726695	44.553652
3502.508574	711716.369851	44.558657
3502.619196	711675.799501	44.563661
3502.544982	711658.687482	44.568666
3502.491150	711617.548323	44.573671
3502.578606	711599.019739	44.578676
3502.617735	711577.322365	44.583681
3502.806095	711542.694907	44.588685
3502.615846	711508.129691	44.593690
3502.805021	711482.386790	44.598695
3502.977049	711451.285856	44.603700
3502.571107	711432.738934	44.608705
3502.735134	711393.846098	44.613709
3502.547603	711369.852592	44.618714
3502.617638	711342.788691	44.623719
3502.486175	711309.255368	44.628724
3502.563282	711287.799187	44.633729
3502.716392	711254.020205	44.638733
3502.645287	711233.829259	44.643738
3502.712796	711203.737405	44.648743
3502.798294	711176.422236	44.653748
3502.524276	711146.684285	44.658753
3502.201527	711119.287284	44.663757
3502.468938	711093.182844	44.668762
3502.530499	711065.573429	44.673767
3502.568241	711042.385746	44.678772
3502.168252	711008.945124	44.683777
3502.581875	710982.319858	44.688781
3502.441484	710964.274192	44.693786
3502.519390	710938.994740	44.698791
3502.822126	710910.947966	44.703796
3502.490905	710887.572456	44.708801
3502.528248	710851.279304	44.713805
3502.669473	710832.243788	44.718810
3502.208413	710797.968510	44.723815
3502.476572	710778.564474	44.728820
3502.222183	710755.324862	44.733825
3502.628922	710723.785470	44.738829
3502.410190	710701.036246	44.743834
3502.576074	710681.202070	44.748839
3502.725016	710657.002187	44.753844
3502.345918	710636.959857	44.758849
3502.377677	710598.680883	44.763853
3502.310110	710579.331713	44.768858
3502.502985	710566.591621	44.773863
3502.225249	710535.958590	44.778868
3502.356359	710522.781829	44.783873
3502.450700	710481.414194	44.788877
3502.458936	710477.143619	44.793882
3502.473759	710435.143509	44.798887
3502.653547	710417.093568	44.803892
3502.705717	710379.554891	44.808897
3502.583186	710355.994604	44.813901
3502.514537	710325.227076	44.818906
3502.290105	710300.343052	44.823911
3502.148877	710272.466621	44.828916
3501.995659	710258.839865	44.833921
3502.476688	710235.527301	44.838925
3502.170943	710209.464954	44.843930
3502.411915	710191.751965	44.848935
3502.338905	710171.509169	44.853940
3502.266713	710156.230635	44.858945
3502.361886	710117.194385	44.863949
3501.966119	710108.373239	44.868954
3501.962534	710088.714544	44.873959
3502.424712	710054.135211	44.878964
3502.119356	710048.377096	44.883969
3502.119303	710018.143254	44.888973
3502.195420	710001.449938	44.893978
3502.190255	709978.961467	44.898983
3502.326425	709936.243869	44.903988
3502.213936	709927.177275	44.908993
3502.378938	709904.759861	44.913997
3501.956439	709890.084676	44.919002
3502.229128	709879.812708	44.924007
3501.942998	709852.107716	44.929012
3501.955343	709838.999116	44.934017
3502.297216	709817.594902	44.939021
3502.450573	709793.888309	44.944026
3502.500964	709768.510629	44.949031
3502.437061	709755.364819	44.954036
3502.421245	709725.182183	44.959041
3502.547112	709709.175156	44.964045
3502.027817	709680.217202	44.969050
3502.207370	709670.357507	44.974055
3502.394366	709634.530991	44.979060
3502.239106	709631.180586	44.984065
3502.398829	709596.847831	44.989069
3502.402242	709586.173051	44.994074
3502.434997	709549.974414	44.999079
3502.748615	709526.985395	45.004084
3502.336560	709505.952868	45.009089
3502.521739	709473.204164	45.014093
3502.401756	709452.967404	45.019098
3502.165212	709428.480019	45.024103
3502.440875	709403.908165	45.029108
3502.261371	709384.078240	45.034113
3502.247482	709354.241518	45.039117
3502.473712	709335.685152	45.044122
3502.232111	709315.269508	45.049127
3502.011837	709289.637109	45.054132
3502.405924	709270.407500	45.059137
3502.491257	709240.405083	45.064141
3502.116662	709225.621558	45.069146
3502.178176	709200.041759	45.074151
3502.419617	709169.864423	45.079156
3502.462066	709159.133028	45.084161
3502.450438	709125.869271	45.089165
3502.520728	709105.600336	45.094170
3502.173570	709089.074285	45.099175
3502.198570	709055.158759	45.104180
3502.148934	709050.102592	45.109185
3502.371965	709005.379997	45.114189
3502.469003	708997.469518	45.119194
3502.286872	708976.397799	45.124199
3502.116627	708949.067991	45.129204
3502.271329	708923.323055	45.134209
3502.356425	708899.228019	45.139213
3502.477894	708884.660075	45.144218
3502.206674	708862.113200	45.149223
3502.429929	708840.229570	45.154228
3502.121854	708823.249695	45.159233
3502.292910	708788.067741	45.164237
3502.134411	708777.220020	45.169242
3502.339673	708754.197130	45.174247
3502.450126	708729.551259	45.179252
3502.437004	708706.713183	45.184257
3502.048508	708692.427552	45.189261
3502.263336	708674.169550	45.194266
3502.090941	708642.916527	45.199271
3502.252195	708626.504420	45.204276
3501.877424	708596.972787	45.209281
3502.367944	708585.719962	45.214285
3502.218949	708573.529771	45.219290
3501.925971	708536.288137	45.224295
3502.284306	708530.419633	45.229300
3502.102631	708497.231106	45.234305
3502.357871	708472.262715	45.239309
3502.096508	708466.446622	45.244314
3502.292707	708446.056072	45.249319
3502.840184	708430.771656	45.254324
3502.439021	708403.031262	45.259329
3502.549705	708364.977551	45.264333
3502.338680	708339.042849	45.269338
3502.721262	708317.330252	45.274343
3502.586039	708284.927730	45.279348
3502.164642	708262.056430	45.284353
3502.125325	708236.142778	45.289357
3502.040372	708225.182927	45.294362
3502.313100	708204.729538	45.299367
3502.402686	708169.260534	45.304372
3501.943101	708157.567831	45.309377
3502.359916	708131.975954	45.314381
3502.359884	708110.524504	45.319386
3502.315665	708093.996266	45.324391
3502.409142	708066.669842	45.329396
3502.384491	708051.181085	45.334401
3502.442826	708025.846587	45.339405
3502.469920	708014.222466	45.344410
3502.395254	707987.022808	45.349415
3502.359915	707963.242927	45.354420
3502.238111	707938.583396	45.359425
3502.551152	707911.567901	45.364429
3502.330714	707892.386808	45.369434
3502.516638	707861.121548	45.374439
3502.405402	707835.466825	45.379444
3502.112581	707818.879703	45.384449
3502.204609	707799.299310	45.389453
3502.109868	707778.359216	45.394458
3502.194200	707762.603689	45.399463
3502.457657	707739.220879	45.404468
3501.905047	707716.022129	45.409473
3502.264344	707696.943708	45.414477
3502.087682	707675.420957	45.419482
3502.140332	707656.740585	45.424487
3502.291577	707645.045848	45.429492
3502.101503	707618.708241	45.434497
3502.224041	707600.562482	45.439501
3502.211754	707573.847827	45.444506
3502.327802	707550.190836	45.449511
3502.326161	707535.094632	45.454516
3502.013286	707509.720457	45.459521
3502.400978	707484.181112	45.464525
3502.398681	707467.793740	45.469530
3502.293114	707439.753217	45.474535
3502.479080	707427.357221	45.479540
3502.089393	707399.859986	45.484545
3502.149947	707380.631447	45.489549
3502.504883	707343.675155	45.494554
3502.394289	707332.718388	45.499559
3502.236898	707305.828165	45.504564
3502.377333	707300.392020	45.509569
3502.262012	707264.605415	45.514573
3502.282644	707242.204828	45.519578
3502.368925	707225.454769	45.524583
3502.321094	707200.036005	45.529588
3501.985556	707193.982958	45.534593
3502.453944	707155.864948	45.539597
3502.160978	707132.969468	45.544602
3502.141640	707116.286262	45.549607
3502.216929	707088.115467	45.554612
3502.045762	707080.793700	45.559617
3502.499601	707045.458685	45.564621
3502.129633	707045.867323	45.569626
3502.399982	707019.551337	45.574631
3502.389512	706985.186507	45.579636
3502.047948	706969.003074	45.584641
3502.215985	706946.229787	45.589645
3501.977051	706926.999918	45.594650
3501.846774	706919.422960	45.599655
3502.121872	706892.112537	45.604660
3502.079824	706877.518470	45.609665
3502.321942	706861.983611	45.614669
3502.339823	706830.692630	45.619674
3502.160304	706801.420617	45.624679
3502.356746	706793.392402	45.629684
3502.322821	706776.611612	45.634689
3502.557521	706751.095304	45.639693
3502.228401	706720.953712	45.644698
3502.309276	706701.620978	45.649703
3502.372860	706677.473587	45.654708
3502.383832	706668.730848	45.659713
3502.362111	706627.910039	45.664717
3502.537087	706610.945511	45.669722
3502.776443	706582.944688	45.674727
3502.573861	706566.091948	45.679732
3502.324708	706525.457124	45.684737
3502.444004	706506.018289	45.689741
3502.841652	706477.146727	45.694746
3502.730073	706458.540479	45.699751
3502.634526	706417.929503	45.704756
3502.439051	706400.429608	45.709761
3502.828519	706368.281060	45.714765
3502.566842	706344.335328	45.719770
3502.375891	706324.549872	45.724775
3502.315381	706294.511525	45.729780
3502.366694	706280.795064	45.734785
3502.224413	706252.558051	45.739789
3502.155004	706229.474325	45.744794
3502.273017	706209.041689	45.749799
3502.382258	706192.434839	45.754804
3502.329918	706166.666094	45.759809
3502.426903	706147.081124	45.764813
3502.065714	706099.260936	45.769818
3502.321778	706012.647163	45.774823
3502.036027	705881.866678	45.779828
3502.090644	705697.632788	45.784833
3502.207256	705441.013369	45.789837
3501.857233	705144.823917	45.794842
3501.739551	704791.062044	45.799847
3501.635965	704370.566261	45.804852
3501.103063	703902.278551	45.809857
3500.852867	703361.480486	45.814861
3499.995648	702781.645179	45.819866
3499.810500	702128.913551	45.824871
3499.370773	701442.432342	45.829876
3498.949009	700685.321930	45.834881
3498.867321	699876.497753	45.839885
3498.195218	699011.326951	45.844890
3497.565219	698083.027147	45.849895
3497.205526	697089.900229	45.854900
3496.144104	696044.913839	45.859905
3495.903363	694946.655185	45.864909
3494.980478	693769.488823	45.869914
3494.106053	692549.278695	45.874919
3493.141988	691275.582526	45.879924
3491.961825	689953.623600	45.884929
3491.340838	688558.718436	45.889933
3490.629098	687121.154414	45.894938
3489.418083	685619.821564	45.899943
3488.554377	684055.794444	45.904948
3487.469797	682439.992016	45.909953
3486.210357	680766.353503	45.914957
3484.948662	679039.054789	45.919962
3483.838742	677268.206843	45.924967
3482.978537	675434.333305	45.929972
3481.164423	673552.601413	45.934977
3479.888882	671608.528518	45.939981
3478.491372	669623.780303	45.944986
3476.753303	667582.308156	45.949991
3475.613284	665503.879552	45.954996
3473.955243	663368.696294	45.960001
3472.640107	661189.858302	45.965005
3470.628582	658958.573878	45.970010
3469.110387	656681.555113	45.975015
3467.401874	654362.382546	45.980020
3465.653419	651989.264634	45.985025
3463.683367	649568.542832	45.990029
3462.025342	647111.445008	45.995034
3460.065902	644611.850281	46.000039
3458.414356	642064.180186	46.005044
3456.048293	639490.731482	46.010049
3454.711014	636860.931553	46.015053
3452.060176	634194.496945	46.020058
3450.278556	631484.387055	46.025063
3448.529242	628727.707335	46.030068
3446.168175	625955.086046	46.035073
3443.721176	623115.729599	46.040077
3441.641040	620265.192143	46.045082
3439.179201	617367.353870	46.050087
3436.951100	614420.227387	46.055092
3434.505753	611460.817231	46.060097
3432.155506	608455.006694	46.065101
3429.571762	605422.089188	46.070106
3427.314300	602353.626429	46.075111
3425.072385	599259.138112	46.080116
3422.183827	596121.897037	46.085121
3419.805382	592951.431816	46.090125
3417.226602	589756.182563	46.095130
3414.382757	586516.497151	46.100135
3411.605773	583260.497953	46.105140
3408.679006	579984.395214	46.110145
3406.240416	576667.454039	46.115149
3403.418043	573337.266949	46.120154
3400.695263	569977.045079	46.125159
3398.073344	566583.552902	46.130164
3394.535271	563172.753411	46.135169
3391.980288	559726.500650	46.140173
3389.217570	556265.478942	46.145178
3386.120399	552785.072627	46.150183
3383.271723	549272.731576	46.155188
3380.131738	545751.976626	46.160193
3377.118228	542184.920264	46.165197
3373.839593	538620.686432	46.170202
3370.619325	535027.599359	46.175207
3367.743006	531391.925376	46.180212
3364.484841	527768.689722	46.185217
3361.220667	524110.134942	46.190221
3358.346424	520448.507146	46.195226
3354.933825	516756.134298	46.200231
3351.733610	513047.689277	46.205236
3348.036896	509334.157574	46.210241
3345.243686	505583.924055	46.215245
3341.666658	501836.595424	46.220250
3338.272988	498065.980627	46.225255
3335.417841	494275.661678	46.230260
3331.580640	490484.612124	46.235265
3328.179288	486667.103985	46.240269
3324.664603	482843.625479	46.245274
3321.084009	479004.913661	46.250279
3317.788619	475158.360088	46.255284
3314.010963	471313.421266	46.260289
3310.589437	467434.966067	46.265293
3306.562046	463558.568607	46.270298
3303.364700	459676.659183	46.275303
3299.967045	455791.548570	46.280308
3296.020007	451893.217579	46.285313
3292.435713	447976.705787	46.290317
3288.939983	444063.468032	46.295322
3285.181899	440138.309337	46.300327
3281.679760	436217.440513	46.305332
3277.609207	432282.035285	46.310337
3273.895737	428339.562469	46.315341
3270.175387	424404.561948	46.320346
3266.126928	420455.070343	46.325351
3262.856455	416510.108946	46.330356
3258.664786	412560.808188	46.335361
3254.574892	408606.352513	46.340365
3250.977800	404658.629427	46.345370
3246.994773	400703.651486	46.350375
3243.357424	396746.366789	46.355380
3239.369880	392800.347552	46.360385
3236.081519	388839.898246	46.365389
3231.914932	384890.275179	46.370394
3228.083959	380933.680487	46.375399
3224.104026	376964.893238	46.380404
3219.864741	373009.548206	46.385409
3216.134857	369049.254300	46.390413
3212.064461	365110.920758	46.395418
3208.302816	361163.405982	46.400423
3204.453189	357221.389158	46.405428
3200.299189	353280.496109	46.410433
3196.476885	349330.129626	46.415437
3192.676918	345399.792917	46.420442
3188.888318	341467.521894	46.425447
3184.866261	337531.360979	46.430452
3180.589298	333593.083902	46.435457
3176.769460	329652.969602	46.440461
3172.574186	325731.915165	46.445466
3168.713501	321812.843143	46.450471
3165.271191	317898.784303	46.455476
3160.619230	313995.012588	46.460481
3156.717457	310079.452856	46.465485
3152.463423	306191.713701	46.470490
3148.612423	302307.448850	46.475495
3144.684543	298414.046072	46.480500
3140.530352	294554.883459	46.485505
3136.438012	290678.822945	46.490509
3132.371298	286819.268737	46.495514
3128.295237	282961.038649	46.500519
3124.089521	279123.241411	46.505524
3120.091222	275292.007777	46.510529
3116.386977	271466.013240	46.515533
3112.323794	267646.703728	46.520538
3107.999852	263845.766781	46.525543
3103.636297	260033.152642	46.530548
3099.417497	256244.092421	46.535553
3095.548075	252473.166406	46.540557
3091.508364	248694.648656	46.545562
3087.260006	244937.897660	46.550567
3083.310051	241187.663526	46.555572
3079.079850	237452.713050	46.560577
3075.122500	233726.371172	46.565581
3071.105160	230009.774462	46.570586
3066.562457	226301.992915	46.575591
3063.099910	222606.134809	46.580596
3058.664569	218930.851019	46.585601
3054.619719	215241.807073	46.590605
3050.725740	211584.148548	46.595610
3046.456675	207900.875539	46.600615
3042.607475	204202.183521	46.605620
3037.900775	200576.445572	46.610625
3034.098698	196959.170535	46.615629
3029.983823	193354.298611	46.620634
3025.598846	189758.141420	46.625639
3021.637584	186180.457098	46.630644
3017.319427	182611.342029	46.635649
3013.420270	179050.563259	46.640653
3009.256743	175519.262026	46.645658
3005.006655	171987.146786	46.650663
3001.090373	168470.646369	46.655668
2996.714208	164977.124102	46.660673
2992.525602	161475.875176	46.665677
2988.640138	158006.905215	46.670682
2984.292982	154544.539053	46.675687
2980.013560	151101.274263	46.680692
2975.510571	147683.152671	46.685697
2971.639317	144263.616830	46.690701
2966.862350	140862.736860	46.695706
2962.815314	137499.441534	46.700711
2959.181607	134131.634735	46.705716
2954.877451	130793.781598	46.710721
2950.794866	127456.507919	46.715725
2946.798294	124127.303563	46.720730
2942.635626	120821.335198	46.725735
2938.244442	117530.052484	46.730740
2934.296724	114261.439551	46.735745
2929.918040	111010.993252	46.740749
2925.722476	107763.934788	46.745754
2921.576906	104528.660944	46.750759
2917.549041	101318.863373	46.755764
2913.116710	98129.555833	46.760769
2909.145499	94944.152957	46.765773
2904.582090	91787.150758	46.770778
2900.216143	88639.534486	46.775783
2896.123422	85510.215141	46.780788
2891.708718	82414.863215	46.785793
2887.620045	79330.033337	46.790797
2882.941013	76259.278696	46.795802
2878.427734	73226.746876	46.800807
2874.304020	70213.963515	46.805812
2869.767160	67214.074652	46.810817
2865.427264	64236.893173	46.815821
2860.731817	61298.716671	46.820826
2855.945908	58374.572430	46.825831
2851.373673	55487.254350	46.830836
2846.172322	52639.729357	46.835841
2841.061517	49806.693440	46.840845
2835.607845	47029.316573	46.845850
2829.529791	44319.488265	46.850855
2820.550638	41720.040448	46.855860
2811.178133	39235.319167	46.860865
2801.943198	36823.539002	46.865869
2793.005222	34520.799738	46.870874
2784.675884	32331.016565	46.875879
2776.118570	30249.863477	46.880884
2767.895508	28278.290376	46.885889
2760.455448	26409.901276	46.890893
2753.461568	24665.075186	46.895898
2746.155594	23021.012317	46.900903
2740.172359	21450.252329	46.905908
2733.427925	19987.421569	46.910913
2727.201707	18599.585408	46.915917
2721.256086	17295.833527	46.920922
2715.528310	16062.599900	46.925927
2710.333311	14910.869116	46.930932
2704.636440	13823.404977	46.935937
2699.090595	12787.446009	46.940941
2693.267857	11842.844190	46.945946
2687.503403	10964.324500	46.950951
2681.769074	10139.886269	46.955956
2676.283946	9381.932808	46.960961
2670.691387	8672.559501	46.965965
2665.322425	8039.632679	46.970970
2660.185926	7451.196673	46.975975
2655.667904	6895.839696	46.980980
2650.684698	6400.843473	46.985985
2646.450700	5930.229238	46.990989
2641.771682	5499.404109	46.995994
2637.591559	5105.251230	47.000999
2633.869023	4728.512619	47.006004
2629.925130	4383.888808	47.011009
2626.477961	4051.723985	47.016013
2623.145892	3746.531314	47.021018
2619.960374	3451.692789	47.026023
2616.734172	3153.421091	47.031028
2613.102534	2865.954002	47.036033
2609.998809	2590.200346	47.041037
2606.905592	2319.115980	47.046042
2603.491566	2056.909856	47.051047
2600.216318	1795.820064	47.056052
2596.933797	1558.892819	47.061057
2593.839453	1284.851262	47.066061
2590.633793	1044.784787	47.071066
2587.056483	799.346416	47.076071
2583.443930	565.115504	47.081076
2579.734351	340.812311	47.086081
2575.003401	152.555712	47.091085
2562.477933	198.746001	47.096090
2553.934880	198.101259	47.101095
2549.408783	192.598906	47.106100
2547.140983	190.770905	47.111105
2545.409864	184.097246	47.116109
2543.460293	179.897388	47.121114
2540.986372	193.224411	47.126119
2538.362367	194.753352	47.131124
2535.166048	187.850661	47.136129
2532.586029	183.132841	47.141133
2529.296929	187.413547	47.146138
2525.220472	191.593908	47.151143
2522.383142	185.418972	47.156148
2518.869807	192.394670	47.161153
2516.056206	187.432028	47.166157
2512.708338	188.357398	47.171162
2509.039065	184.240690	47.176167
2505.696774	188.162545	47.181172
2502.751659	183.414223	47.186177
2499.239836	184.033552	47.191181
2495.873532	191.879343	47.196186
2492.423043	185.862856	47.201191
2488.982392	180.346192	47.206196
2485.991258	190.884144	47.211201
2482.659030	180.906079	47.216205
2478.846223	182.302694	47.221210
2475.454420	190.456805	47.226215
2472.663128	177.456795	47.231220
2468.621298	180.263521	47.236225
2464.820551	179.447552	47.241229
2461.689724	172.870971	47.246234
2458.710301	176.846626	47.251239
2455.390186	169.816824	47.256244
2451.571200	177.685650	47.261249
2447.996533	180.949680	47.266253
2444.764741	176.507824	47.271258
2441.543199	184.880525	47.276263
2438.157671	174.419723	47.281268
2434.430290	182.972421	47.286273
2431.473954	176.022107	47.291277
2428.344817	174.687802	47.296282
2424.313882	181.859502	47.301287
2420.637612	169.738337	47.306292
2416.923190	181.850693	47.311297
2413.790893	171.583737	47.316301
2410.805822	179.354803	47.321306
2407.094965	177.533395	47.326311
2403.584915	171.366968	47.331316
2400.358988	176.195596	47.336321
2396.488399	172.295540	47.341325
2393.150814	169.680989	47.346330
2389.361411	167.100175	47.351335
2386.676137	166.297475	47.356340
2383.101117	169.615677	47.361345
2379.582352	170.452717	47.366349
2375.958925	169.770156	47.371354
2372.551736	174.171289	47.376359
2368.818663	174.857820	47.381364
2365.728883	170.677932	47.386369
2361.749422	176.759955	47.391373
2358.541298	171.567718	47.396378
2354.622965	169.763039	47.401383
2351.679620	168.748589	47.406388
2348.039882	163.244577	47.411393
2344.746240	167.225790	47.416397
2341.606797	165.000282	47.421402
2337.609947	166.317664	47.426407
2334.102425	167.031122	47.431412
2330.728603	172.443467	47.436417
2327.279940	164.531958	47.441421
2323.590539	171.872512	47.446426
2320.378009	173.697836	47.451431
2316.842757	161.400155	47.456436
2313.381364	170.413021	47.461441
2309.871043	165.695976	47.466445
2306.617551	169.252028	47.471450
2302.538659	161.684943	47.476455
2299.353331	160.952019	47.481460
2295.932490	173.176611	47.486465
2292.271290	157.978924	47.491469
2289.164725	165.527377	47.496474
2285.500175	164.506328	47.501479
2282.208076	162.312377	47.506484
2278.667509	177.771211	47.511489
2274.931164	169.866583	47.516493
2271.893778	167.811349	47.521498
2268.274349	164.913665	47.526503
2264.842654	158.845320	47.531508
2260.862470	168.985424	47.536513
2257.822197	164.977411	47.541517
2254.037171	164.522117	47.546522
2250.034147	160.755547	47.551527
2247.277730	163.791673	47.556532
2243.658754	171.850020	47.561537
2240.430201	169.455765	47.566541
2236.876592	163.647927	47.571546
2233.167518	163.212078	47.576551
2229.743724	160.911637	47.581556
2225.997005	157.349051	47.586561
2222.832659	166.071777	47.591565
2218.969160	161.397328	47.596570
2215.625195	170.818302	47.601575
2212.461316	163.408666	47.606580
2208.560612	158.859957	47.611585
2205.369933	167.611708	47.616589
2201.991827	164.471366	47.621594
2198.421794	171.194159	47.626599
2194.953979	161.957825	47.631604
2191.496187	171.192374	47.636609
2187.812296	162.514079	47.641613
2184.098027	163.826762	47.646618
2180.415278	155.702022	47.651623
2177.413790	151.763638	47.656628
2173.711927	159.135946	47.661633
2170.287651	162.820530	47.666637
2167.150183	154.970253	47.671642
2163.565497	170.431693	47.676647
2159.989125	163.899098	47.681652
2156.396276	172.453048	47.686657
2152.749941	168.523468	47.691661
2148.777401	162.492812	47.696666
2145.806845	171.400659	47.701671
2142.879367	157.796834	47.706676
2138.828987	171.557554	47.711681
2135.842844	170.892687	47.716685
2132.298104	163.524883	47.721690
2128.441956	168.549699	47.726695
2125.136312	162.745604	47.731700
2121.494091	162.648684	47.736705
2117.727368	165.575432	47.741709
2114.280080	161.754115	47.746714
2110.855025	162.053910	47.751719
2107.716038	163.806444	47.756724
2103.661866	164.585666	47.761729
2099.867827	161.235636	47.766733
2097.025284	161.451289	47.771738
2093.721914	161.011899	47.776743
2090.205644	151.414239	47.781748
2086.129470	163.278086	47.786753
2082.833958	164.884798	47.791757
2079.549738	155.009454	47.796762
2075.853897	160.610507	47.801767
2072.857437	150.120894	47.806772
2069.200424	162.796849	47.811777
2065.649244	154.795919	47.816781
2062.161031	153.638175	47.821786
2058.559044	163.343981	47.826791
2055.046502	159.656230	47.831796
2051.369912	159.576682	47.836801
2048.019328	154.959366	47.841805
2044.739986	152.083645	47.846810
2040.933059	152.999496	47.851815
2037.529725	149.852392	47.856820
2033.888513	148.046616	47.861825
2030.350005	153.606522	47.866829
2026.957784	149.045632	47.871834
2023.390903	148.509896	47.876839
2020.317403	143.632141	47.881844
2016.457287	150.823680	47.886849
2013.111674	150.519395	47.891853
2009.703108	153.552049	47.896858
2006.022602	162.731726	47.901863
2003.111881	149.633197	47.906868
1999.065435	155.647612	47.911873
1995.526124	147.315623	47.916877
1992.308571	147.695295	47.921882
1987.981165	157.245463	47.926887
1984.700088	146.496061	47.931892
1981.548793	143.178118	47.936897
1978.102909	145.657500	47.941901
1974.558900	147.134429	47.946906
1970.741046	148.866162	47.951911
1967.915410	142.847147	47.956916
1964.364603	144.762902	47.961921
1960.865742	138.081910	47.966925
1957.202032	141.459651	47.971930
1953.526850	148.920251	47.976935
1950.089524	141.386664	47.981940
1946.538571	150.061893	47.986945
1942.990918	151.033471	47.991949
1939.483130	141.362316	47.996954
1936.089248	149.644559	48.001959
1932.731729	137.265777	48.006964
1928.988218	144.045809	48.011969
1925.309201	147.862220	48.016973
1922.104448	143.129943	48.021978
1918.512874	153.362784	48.026983
1915.267614	138.823561	48.031988
1911.528833	149.117619	48.036993
1908.055931	140.466890	48.041997
1904.716055	139.245690	48.047002
1901.023426	145.398287	48.052007
1898.084882	137.886357	48.057012
1894.047280	148.967435	48.062017
1890.425269	139.871091	48.067021
1887.317781	139.150648	48.072026
1883.367471	150.514507	48.077031
1880.209099	139.012604	48.082036
1876.573524	146.113083	48.087041
1873.076158	144.992710	48.092045
1869.611448	146.517002	48.097050
1865.989396	137.608159	48.102055
1862.560746	138.659005	48.107060
1858.898581	146.371493	48.112065
1855.462045	143.376633	48.117069
1852.043279	148.551804	48.122074
1848.535935	144.776331	48.127079
1845.429156	137.194545	48.132084
1841.241330	148.528796	48.137089
1837.821159	140.758028	48.142093
1834.558897	148.868418	48.147098
1830.819717	140.296074	48.152103
1828.033127	136.004715	48.157108
1824.072489	148.508962	48.162113
1820.428858	149.407287	48.167117
1817.017063	130.985998	48.172122
1813.301056	147.607755	48.177127
1810.159852	137.729731	48.182132
1806.288213	141.852347	48.187137
1803.169680	135.674030	48.192141
1799.639729	138.893430	48.197146
1795.928768	139.909458	48.202151
1792.878272	140.535770	48.207156
1789.140674	135.114694	48.212161
1785.137114	130.923364	48.217165
1782.054588	135.025951	48.222170
1778.782319	138.418883	48.227175
1775.447010	133.975478	48.232180
1771.014431	138.002724	48.237185
1767.812596	135.063092	48.242189
1764.616703	133.372421	48.247194
1760.717277	143.055518	48.252199
1757.753884	130.206841	48.257204
1754.169946	138.839093	48.262209
1750.958382	137.977668	48.267213
1747.357582	133.516378	48.272218
1743.610757	127.050978	48.277223
1740.237006	123.985254	48.282228
1736.380483	130.396517	48.287233
1732.834634	124.646032	48.292237
1729.212648	132.034646	48.297242
1725.757466	134.902916	48.302247
1722.849732	129.068132	48.307252
1719.350162	135.427147	48.312257
1715.704852	129.519646	48.317261
1711.879461	123.281564	48.322266
1708.504060	132.920545	48.327271
1704.864398	130.700956	48.332276
1701.368681	133.721180	48.337281
1698.077236	137.447676	48.342285
1694.457411	131.576436	48.347290
1690.939185	130.130883	48.352295
1687.575263	130.204007	48.357300
1683.932109	131.811392	48.362305
1680.446129	121.432962	48.367309
1677.239453	127.148441	48.372314
1673.356830	136.111498	48.377319
1670.019098	119.432455	48.382324
1666.167988	127.408946	48.387329
1662.598762	129.012617	48.392333
1659.714286	129.421943	48.397338
1656.240067	132.086005	48.402343
1652.725911	124.927080	48.407348
1649.299268	133.274702	48.412353
1645.527308	133.258982	48.417357
1642.123498	132.492150	48.422362
1638.328728	141.181024	48.427367
1635.013873	137.939486	48.432372
1630.867825	132.714303	48.437377
1627.649982	129.342091	48.442381
1624.756829	125.357177	48.447386
1620.957562	121.212557	48.452391
1617.443924	134.258183	48.457396
1614.158119	128.290774	48.462401
1610.239776	129.325426	48.467405
1607.155760	129.360449	48.472410
1603.576177	138.536142	48.477415
1600.094990	122.347763	48.482420
1596.594797	125.626128	48.487425
1592.792927	138.209478	48.492429
1589.294912	127.158216	48.497434
1585.645219	129.202674	48.502439
1582.739022	127.661008	48.507444
1578.685712	127.924295	48.512449
1575.685265	120.370141	48.517453
1572.156906	128.392236	48.522458
1568.167392	128.019234	48.527463
1564.636072	118.142926	48.532468
1561.159988	132.875534	48.537473
1557.709923	123.717726	48.542477
1554.703619	128.625030	48.547482
1550.796174	130.124041	48.552487
1547.688594	123.373604	48.557492
1543.910056	127.056564	48.562497
1540.788499	130.300226	48.567501
1537.376046	121.796118	48.572506
1533.350544	129.409022	48.577511
1529.483489	121.776693	48.582516
1526.004387	119.781138	48.587521
1522.725671	127.665713	48.592525
1519.496569	114.894096	48.597530
1516.098651	124.495472	48.602535
1512.772352	123.613707	48.607540
1508.777442	121.114352	48.612545
1505.180166	126.644460	48.617549
1502.201227	123.396059	48.622554
1498.573734	130.152881	48.627559
1495.204212	121.373334	48.632564
1491.179390	126.155750	48.637569
1487.924981	125.235087	48.642573
1484.355049	121.823288	48.647578
1480.462269	132.726212	48.652583
1477.272361	120.078984	48.657588
1474.033815	126.113030	48.662593
1470.051346	125.877874	48.667597
1467.017549	121.807971	48.672602
1462.943115	122.606871	48.677607
1459.328745	114.379715	48.682612
1456.078041	129.778839	48.687617
1452.984561	115.010702	48.692621
1449.521490	124.625453	48.697626
1446.081725	125.205220	48.702631
1442.759824	121.506975	48.707636
1438.905137	122.360355	48.712641
1435.327221	121.885304	48.717645
1431.813549	119.370225	48.722650
1427.841905	117.715449	48.727655
1425.012052	118.096355	48.732660
1421.400521	111.796353	48.737665
1417.617734	119.315356	48.742669
1414.469793	120.667246	48.747674
1410.353853	122.256875	48.752679
1407.347773	126.029937	48.757684
1403.436501	123.261300	48.762689
1399.865050	120.259295	48.767693
1397.143152	121.593076	48.772698
1393.839585	130.051748	48.777703
1389.898441	127.498027	48.782708
1386.540210	125.909639	48.787713
1382.851897	127.460189	48.792717
1379.014045	124.072825	48.797722
1375.387705	126.476289	48.802727
1371.953128	123.031354	48.807732
1369.066067	122.302257	48.812737
1365.349916	121.734273	48.817741
1361.979103	127.266718	48.822746
1358.271666	123.942079	48.827751
1354.524843	124.139710	48.832756
1351.265812	121.850193	48.837761
1347.472555	117.279754	48.842765
1344.377161	113.643013	48.847770
1340.607046	119.707974	48.852775
1337.683151	120.415481	48.857780
1333.610237	125.883235	48.862785
1330.175374	123.440852	48.867789
1326.994350	122.829636	48.872794
1323.146081	124.721030	48.877799
1319.963682	117.609968	48.882804
1316.107541	121.275542	48.887809
1312.279585	117.451869	48.892813
1309.308281	118.904085	48.897818
1305.867856	121.489994	48.902823
1302.365344	119.343376	48.907828
1298.768727	114.063808	48.912833
1295.142149	119.445776	48.917837
1291.819883	121.578812	48.922842
1287.914787	122.119188	48.927847
1284.659340	118.408303	48.932852
1281.185356	127.014999	48.937857
1277.546269	117.449208	48.942861
1273.882621	116.887617	48.947866
1270.627909	126.128031	48.952871
1267.248805	111.274262	48.957876
1263.865440	118.985864	48.962881
1260.115616	117.870792	48.967885
1256.814193	116.200492	48.972890
1252.806433	118.095219	48.977895
1250.086910	107.224410	48.982900
1246.306177	113.395587	48.987905
1242.674910	114.540761	48.992909
1239.099653	112.585993	48.997914
1235.515351	119.779472	49.002919
1232.290704	115.093232	49.007924
1228.545243	121.404229	49.012929
1225.097922	112.659282	49.017933
1221.748212	115.632427	49.022938
1217.732857	116.471702	49.027943
1214.605647	108.942721	49.032948
1210.853972	113.327765	49.037953
1207.674399	114.778561	49.042957
1204.677098	113.614512	49.047962
1200.622449	120.202200	49.052967
1197.372096	115.125563	49.057972
1193.374975	108.954822	49.062977
1189.791550	124.814420	49.067981
1186.885883	113.301902	49.072986
1182.829451	123.846300	49.077991
1179.741479	113.044344	49.082996
1176.047707	116.775145	49.088001
1172.747322	112.189682	49.093005
1169.560694	111.770132	49.098010
1165.111727	117.613960	49.103015
1162.003413	114.296408	49.108020
1158.508644	116.836549	49.113025
1155.029814	118.971096	49.118029
1151.953938	112.202695	49.123034
1148.169998	120.192737	49.128039
1144.723601	111.522694	49.133044
1141.108472	116.677129	49.138049
1137.609152	124.402659	49.143053
1134.059288	114.424813	49.148058
1130.705459	119.396340	49.153063
1127.119932	113.655882	49.158068
1123.256815	111.849641	49.163073
1120.108059	112.631562	49.168077
1116.783017	108.792797	49.173082
1112.695226	120.071787	49.178087
1109.563032	114.533056	49.183092
1105.811161	118.867698	49.188097
1102.679612	114.707852	49.193101
1099.470844	108.660429	49.198106
1095.428761	117.681847	49.203111
1092.239817	109.931691	49.208116
1088.130364	116.705148	49.213121
1084.899985	109.318633	49.218125
1081.581643	113.288961	49.223130
1077.823390	115.409185	49.228135
1074.578359	113.388700	49.233140
1070.862761	108.411586	49.238145
1067.513119	108.203769	49.243149
1064.384337	109.876556	49.248154
1060.666704	118.593145	49.253159
1056.960723	111.379422	49.258164
1053.450036	118.184933	49.263169
1049.956803	110.463023	49.268173
1046.820157	113.913345	49.273178
1042.535125	112.840778	49.278183
1039.662154	112.661908	49.283188
1035.482169	113.319981	49.288193
1032.482869	112.755886	49.293197
1029.075576	113.975885	49.298202
1025.450719	122.089296	49.303207
1022.039952	115.602713	49.308212
1018.503613	118.372033	49.313217
1014.829153	120.579488	49.318221
1011.201741	119.427017	49.323226
1007.691301	118.152197	49.328231
1004.291369	109.265811	49.333236
1000.713820	117.007526	49.338241
997.961064	109.964990	49.343245
994.498607	107.565719	49.348250
990.413385	125.966638	49.353255
986.814794	116.048879	49.358260
983.191070	118.614818	49.363265
979.681085	114.924354	49.368269
976.454425	114.224831	49.373274
972.786957	120.417155	49.378279
969.203418	111.852823	49.383284
966.141939	117.401672	49.388289
962.696085	113.282462	49.393293
959.155796	108.093525	49.398298
955.519388	110.980082	49.403303
952.146074	106.337787	49.408308
948.231492	109.262853	49.413313
944.740730	108.823310	49.418317
941.509496	102.690335	49.423322
937.882394	117.005852	49.428327
934.083400	104.287942	49.433332
930.470958	107.623637	49.438337
927.077181	106.926925	49.443341
924.058376	110.760799	49.448346
920.571403	109.802247	49.453351
917.101416	99.915193	49.458356
913.473215	108.544870	49.463361
909.903387	109.784142	49.468365
906.183622	108.501596	49.473370
903.090202	110.786897	49.478375
899.892749	118.221916	49.483380
895.915882	119.482539	49.488385
892.107454	110.390103	49.493389
888.563762	105.925026	49.498394
885.388267	110.198060	49.503399
881.979057	104.656382	49.508404
878.118961	107.191638	49.513409
874.652897	118.321613	49.518413
871.400141	109.982285	49.523418
867.384587	117.369308	49.528423
864.454423	101.799927	49.533428
861.024767	112.439624	49.538433
857.447778	105.751765	49.543437
854.032720	103.793707	49.548442
850.325244	109.442959	49.553447
847.143896	103.402251	49.558452
843.271327	107.853558	49.563457
839.723245	114.263234	49.568461
836.384958	113.533535	49.573466
832.409141	122.121316	49.578471
829.323404	106.867380	49.583476
825.191557	115.342441	49.588481
822.200192	105.770777	49.593485
818.961976	100.791889	49.598490
814.980650	109.014925	49.603495
811.908617	111.022059	49.608500
808.368715	109.530073	49.613505
804.970382	103.901015	49.618509
801.648569	92.855275	49.623514
797.819190	107.537831	49.628519
794.341264	101.645087	49.633524
790.771432	108.804915	49.638529
786.913638	105.113536	49.643533
783.740378	102.525702	49.648538
779.989360	106.429871	49.653543
776.826557	97.655227	49.658548
772.914782	100.477954	49.663553
769.897363	102.852400	49.668557
766.303015	99.453723	49.673562
762.415164	106.978953	49.678567
759.272131	94.566727	49.683572
755.795300	104.382918	49.688577
752.425108	106.764029	49.693581
748.872885	102.496634	49.698586
745.089883	110.428017	49.703591
741.674322	106.293717	49.708596
738.198688	92.364952	49.713601
734.919639	105.406642	49.718605
731.637106	97.186817	49.723610
727.354184	102.703631	49.728615
723.759492	104.200345	49.733620
720.287223	109.616217	49.738625
717.245397	107.836878	49.743629
713.534651	101.971272	49.748634
710.177930	114.693127	49.753639
706.891232	108.518599	49.758644
703.430006	107.014078	49.763649
699.788921	103.517811	49.768653
696.697937	96.561834	49.773658
692.780303	114.026697	49.778663
689.184516	98.852139	49.783668
685.462128	104.474385	49.788673
681.899273	97.213258	49.793677
678.634041	93.484927	49.798682
674.794261	102.980754	49.803687
671.657385	94.542509	49.808692
668.260688	106.025023	49.813697
664.576504	99.343033	49.818701
661.552851	100.367822	49.823706
657.384894	104.929128	49.828711
653.811558	106.561091	49.833716
650.039973	103.841068	49.838721
646.941159	114.258042	49.843725
643.533631	108.243467	49.848730
640.181792	112.719102	49.853735
637.143207	97.726311	49.858740
633.369279	103.434086	49.863745
629.788511	107.933394	49.868749
626.300825	105.392567	49.873754
622.187616	98.505526	49.878759
618.841527	104.352294	49.883764
615.446046	97.434722	49.888769
611.803473	98.179904	49.893773
608.758640	100.783362	49.898778
605.365018	106.096319	49.903783
601.870833	108.053856	49.908788
598.170275	109.719148	49.913793
594.312118	104.539309	49.918797
590.921931	101.227771	49.923802
587.492022	114.600389	49.928807
584.252823	103.932280	49.933812
580.578918	111.144608	49.938817
576.612268	107.928066	49.943821
573.701554	100.599782	49.948826
569.693694	106.525100	49.953831
566.644409	105.130723	49.958836
563.251028	110.363751	49.963841
559.595132	106.992404	49.968845
556.342702	103.538317	49.973850
551.904375	105.357887	49.978855
549.048973	104.281514	49.983860
545.733399	109.137795	49.988865
542.070071	105.887278	49.993869
538.541762	105.549584	49.998874
534.798513	102.793006	50.003879
531.596804	99.633456	50.008884
527.987678	95.958398	50.013889
524.222790	106.304305	50.018893
520.755368	105.760794	50.023898
517.453837	106.022786	50.028903
514.092795	108.421702	50.033908
510.984181	103.547709	50.038913
507.322862	105.899228	50.043917
503.646166	88.888829	50.048922
499.699269	111.927061	50.053927
496.620116	105.264491	50.058932
493.074149	108.414691	50.063937
489.421329	103.910983	50.068941
485.869718	97.090793	50.073946
482.079841	107.276488	50.078951
478.778530	101.596128	50.083956
475.464663	102.539420	50.088961
471.854428	103.601813	50.093965
468.792748	94.767472	50.098970
465.059856	122.019140	50.103975
461.654774	107.148907	50.108980
457.858064	106.706510	50.113985
454.305955	107.393044	50.118989
450.990919	101.050158	50.123994
447.189162	106.206796	50.128999
443.846585	109.766590	50.134004
440.511394	100.792628	50.139009
436.654835	97.400529	50.144013
433.461722	106.076953	50.149018
429.849592	110.379733	50.154023
426.386335	106.717522	50.159028
422.911058	102.315325	50.164033
419.365307	106.150298	50.169037
416.348480	98.991839	50.174042
412.397289	108.649774	50.179047
408.787549	106.317781	50.184052
405.227987	102.053475	50.189057
401.497425	110.876491	50.194061
398.403405	100.577016	50.199066
394.963253	110.743973	50.204071
391.680118	100.067714	50.209076
388.366628	104.258546	50.214081
384.196058	110.887220	50.219085
380.824898	99.083366	50.224090
377.139196	99.656110	50.229095
373.446111	95.843529	50.234100
370.257635	92.382756	50.239105
367.083902	100.933271	50.244109
363.715726	99.047373	50.249114
359.870972	105.513016	50.254119
356.226656	92.084357	50.259124
352.776916	105.247477	50.264129
348.849398	97.254705	50.269133
345.770990	95.474784	50.274138
342.127711	100.458657	50.279143
338.799118	90.882814	50.284148
335.488210	94.786725	50.289153
331.928713	103.290014	50.294157
328.515463	100.635882	50.299162
324.754404	109.849399	50.304167
321.434650	93.953651	50.309172
317.927139	98.394898	50.314177
314.160207	98.131221	50.319181
311.185342	94.053790	50.324186
307.309820	98.825714	50.329191
303.733414	93.503417	50.334196
300.100540	98.797784	50.339201
296.681922	96.757291	50.344205
293.379857	89.452759	50.349210
289.775170	88.377252	50.354215
286.323350	87.188237	50.359220
283.072611	90.910348	50.364225
279.215417	93.996987	50.369229
275.615696	93.209173	50.374234
271.993565	97.050192	50.379239
268.463655	105.601123	50.384244
265.053167	97.799711	50.389249
261.453303	104.878864	50.394253
258.576960	82.508855	50.399258
254.477302	100.383028	50.404263
251.572024	97.074381	50.409268
248.014158	98.225378	50.414273
244.085385	95.295729	50.419277
240.779571	93.612137	50.424282
236.932358	105.577994	50.429287
233.447028	92.469461	50.434292
230.542912	96.259933	50.439297
226.603747	97.847423	50.444301
223.368211	91.290094	50.449306
219.689728	108.128038	50.454311
216.104305	103.091865	50.459316
212.615258	101.698121	50.464321
208.871574	99.314673	50.469325
205.829708	97.803691	50.474330
202.105583	106.955342	50.479335
198.697364	98.205422	50.484340
195.209637	102.389717	50.489345
191.721726	108.239746	50.494349
188.575345	98.583545	50.499354
184.575167	101.965667	50.504359
181.048883	99.598548	50.509364
177.559618	96.584559	50.514369
174.050893	103.495559	50.519373
170.702856	98.598715	50.524378
167.162103	101.479933	50.529383
163.603303	106.232108	50.534388
160.240193	102.578210	50.539393
156.441394	100.379364	50.544397
153.404536	100.214002	50.549402
149.698971	100.884949	50.554407
146.353965	99.638108	50.559412
142.591371	93.254930	50.564417
138.911949	105.355686	50.569421
135.809502	96.004243	50.574426
131.776826	106.696114	50.579431
128.100259	97.717576	50.584436
125.015662	97.750763	50.589441
121.821467	95.106909	50.594445
118.672125	101.970881	50.599450
114.714380	110.528430	50.604455
111.026179	99.914749	50.609460
107.654639	103.576674	50.614465
103.892949	94.246002	50.619469
100.577896	96.616106	50.624474
96.835255	105.015508	50.629479
93.726725	99.653030	50.634484
90.069477	98.774653	50.639489
86.558478	104.028884	50.644493
83.381725	98.431437	50.649498
79.574994	85.918744	50.654503
75.877932	100.117951	50.659508
72.657597	103.960686	50.664513
69.125010	100.596985	50.669517
65.676579	100.242904	50.674522
61.905246	94.789904	50.679527
58.300794	96.777967	50.684532
54.959340	93.515636	50.689537
51.595879	92.057031	50.694541
48.013782	93.743229	50.699546
44.607372	104.835662	50.704551
41.462844	97.303580	50.709556
37.808580	95.850119	50.714561
33.610062	97.856453	50.719565
30.653597	91.377000	50.724570
26.789300	102.696618	50.729575
23.524463	93.573835	50.734580
20.074503	97.263414	50.739585
16.344565	102.524353	50.744589
13.170029	93.645923	50.749594
9.435310	108.618851	50.754599
5.909632	100.619281	50.759604
2.428403	95.676555	50.764609