Tue Jun 21 11:16:20 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.531424	94.595365	0.000000
0.524263	86.633385	0.005005
0.888620	84.722494	0.010010
0.400363	82.117280	0.015014
0.905925	87.006408	0.020019
0.664598	85.310268	0.025024
0.254535	75.082925	0.030029
0.287163	68.490570	0.035034
-0.211958	71.168985	0.040038
-0.182472	51.446201	0.045043
-0.705768	54.017716	0.050048
-1.228573	46.264677	0.055053
-1.469563	32.244249	0.060058
-1.556801	34.759535	0.065062
-1.626346	29.316215	0.070067
-1.653117	31.259483	0.075072
-2.396793	24.015249	0.080077
-2.628959	18.988200	0.085082
-3.140369	16.659547	0.090086
-2.935734	16.192357	0.095091
-3.334332	10.970280	0.100096
-3.713630	1.103353	0.105101
-3.609959	-2.601921	0.110106
-4.599805	-2.617737	0.115110
-4.427765	-5.771736	0.120115
-4.762286	-8.726411	0.125120
-5.368818	-5.242273	0.130125
-4.920654	-13.401749	0.135130
-5.655041	-8.823149	0.140134
-6.192308	-15.403974	0.145139
-6.438860	-15.556295	0.150144
-6.552117	-5.238526	0.155149
-6.470277	-19.313155	0.160154
-6.641223	-9.435951	0.165158
-6.948203	-15.140868	0.170163
-7.978162	-12.489013	0.175168
-8.319114	-7.286085	0.180173
-8.242809	-20.643084	0.185178
-8.048813	-11.389501	0.190182
-7.918037	-26.457705	0.195187
-8.251093	-15.330989	0.200192
-8.590255	-16.992169	0.205197
-9.219587	-19.190387	0.210202
-9.825222	-5.541019	0.215206
-9.759872	-14.756569	0.220211
-9.886932	-15.147914	0.225216
-9.854851	-26.344491	0.230221
-9.457755	-14.645854	0.235226
-10.675400	-24.994347	0.240230
-11.008570	-22.629954	0.245235
-11.263687	-16.821620	0.250240
-11.237252	-27.450523	0.255245
-11.324663	-21.790138	0.260250
-12.087190	-13.184457	0.265254
-12.724256	-14.505633	0.270259
-12.354197	-20.628135	0.275264
-12.772456	-19.664523	0.280269
-12.101107	-20.383836	0.285274
-13.124383	-7.046357	0.290278
-13.607473	-10.709715	0.295283
-13.917239	-11.534535	0.300288
-14.137217	-15.837801	0.305293
-14.066527	-15.578333	0.310298
-14.056115	-13.431267	0.315302
-14.342942	-12.276893	0.320307
-15.116476	-24.345470	0.325312
-15.772595	-16.905886	0.330317
-15.662338	-21.017961	0.335322
-15.976247	-13.643332	0.340326
-15.740185	-25.655322	0.345331
-15.827568	-21.311739	0.350336
-16.286618	-10.918754	0.355341
-15.931167	-23.028266	0.360346
-17.085130	-9.050313	0.365350
-17.188277	-25.859322	0.370355
-17.236695	-17.625076	0.375360
-17.701431	-16.178591	0.380365
-17.574645	-19.463227	0.385370
-18.931959	-19.017799	0.390374
-18.795103	-16.799716	0.395379
-18.891176	-17.174682	0.400384
-19.007412	-14.149629	0.405389
-18.907860	-12.586628	0.410394
-19.188421	-11.011592	0.415398
-19.427090	-10.301889	0.420403
-20.010869	-14.699617	0.425408
-20.570323	-11.550649	0.430413
-20.455670	-25.841850	0.435418
-20.674105	-8.833089	0.440422
-20.780668	-18.226182	0.445427
-20.648585	-13.888551	0.450432
-21.718812	-15.258170	0.455437
-21.799697	-32.254771	0.460442
-22.296894	-9.075250	0.465446
-22.393893	-14.751397	0.470451
-22.502530	-22.598637	0.475456
-22.747847	-13.405703	0.480461
-22.775467	-20.392573	0.485466
-22.729753	-17.431832	0.490470
-22.979303	-17.477491	0.495475
-23.697007	-9.948574	0.500480
-23.756603	-17.355796	0.505485
-23.847731	-26.815177	0.510490
-24.852380	-20.192847	0.515494
-25.118270	-28.694838	0.520499
-25.291301	-16.588625	0.525504
-25.263505	-16.825252	0.530509
-25.246350	-22.977716	0.535514
-25.651662	-9.004156	0.540518
-25.411599	-15.600436	0.545523
-25.989466	-19.661703	0.550528
-26.842668	-13.469178	0.555533
-26.960153	-20.042751	0.560538
-27.391891	-14.254106	0.565542
-27.301222	-24.791626	0.570547
-27.189087	-16.108398	0.575552
-27.322665	-20.018083	0.580557
-27.505742	-18.559041	0.585562
-28.564699	-16.178251	0.590566
-28.447330	-16.704003	0.595571
-28.504336	-18.451176	0.600576
-28.745893	-16.540622	0.605581
-29.234101	-21.004493	0.610586
-30.038370	-20.258154	0.615590
-30.278263	-24.697237	0.620595
-30.014771	-26.237598	0.625600
-30.421093	-19.020728	0.630605
-30.328222	-23.952403	0.635610
-30.561151	-21.695382	0.640614
-30.407998	-25.977556	0.645619
-31.054181	-20.088082	0.650624
-31.609333	-10.625785	0.655629
-31.777508	-15.768989	0.660634
-32.193171	-18.667005	0.665638
-32.028043	-22.249844	0.670643
-32.114619	-14.965354	0.675648
-32.542118	-14.300549	0.680653
-32.910122	-22.013669	0.685658
-33.440630	-13.790754	0.690662
-33.526962	-21.246430	0.695667
-33.352177	-12.634157	0.700672
-33.710249	-9.523273	0.705677
-34.563749	-22.622492	0.710682
-34.854800	-12.460384	0.715686
-34.818825	-23.494610	0.720691
-35.391987	-20.263650	0.725696
-35.498042	-15.719443	0.730701
-35.291034	-20.481569	0.735706
-35.843720	-15.055521	0.740710
-35.528756	-24.968726	0.745715
-35.432644	-31.941547	0.750720
-36.347020	-24.335272	0.755725
-36.734939	-27.412519	0.760730
-36.904430	-21.291782	0.765734
-36.833654	-27.886070	0.770739
-37.400951	-28.739080	0.775744
-37.933659	-20.674657	0.780749
-37.926773	-25.002858	0.785754
-38.590418	-21.995094	0.790758
-38.326229	-22.695330	0.795763
-38.674715	-14.928995	0.800768
-39.521132	-14.448584	0.805773
-39.460465	-22.654194	0.810778
-39.919460	-16.718560	0.815782
-39.731896	-13.746186	0.820787
-39.870674	-16.468057	0.825792
-40.221878	-17.034611	0.830797
-39.792044	-17.999669	0.835802
-40.644711	-19.221793	0.840806
-41.008158	-14.647985	0.845811
-41.498613	-13.417855	0.850816
-41.637129	-14.619127	0.855821
-41.280451	-14.295331	0.860826
-41.650256	-15.098366	0.865830
-42.324335	-17.657390	0.870835
-42.398309	-10.934620	0.875840
-42.933438	-11.953587	0.880845
-43.084612	-14.733591	0.885850
-43.065197	-16.647338	0.890854
-43.270564	-9.814008	0.895859
-43.728389	-22.562773	0.900864
-44.385701	-15.703145	0.905869
-44.431311	-17.780960	0.910874
-44.702049	-15.695275	0.915878
-44.634731	-24.399657	0.920883
-44.403997	-15.622210	0.925888
-45.665422	-17.378503	0.930893
-45.966327	-19.404370	0.935898
-46.230307	-15.418509	0.940902
-46.427879	-12.725909	0.945907
-46.525794	-14.118607	0.950912
-46.628169	-8.752330	0.955917
-46.419804	-15.271532	0.960922
-46.703795	-6.514214	0.965926
-46.951011	-14.831442	0.970931
-46.963348	-17.182547	0.975936
-47.738103	-3.219827	0.980941
-47.599095	-17.711213	0.985946
-48.248786	-12.154448	0.990950
-48.341514	-17.571412	0.995955
-48.962520	-15.233743	1.000960
-49.612566	-12.325118	1.005965
-49.413562	-18.079092	1.010970
-49.701201	-15.284553	1.015974
-49.548311	-13.125366	1.020979
-49.452781	-24.975948	1.025984
-50.000137	-8.713099	1.030989
-50.499850	-18.326816	1.035994
-51.331553	-13.544629	1.040998
-51.244674	-26.660059	1.046003
-50.843677	-15.273467	1.051008
-51.124395	-17.850668	1.056013
-51.256157	-20.650264	1.061018
-52.339342	-10.396044	1.066022
-52.900478	-18.907748	1.071027
-52.729214	-19.044605	1.076032
-52.719787	-14.769149	1.081037
-52.259448	-21.762629	1.086042
-52.855054	-16.371109	1.091046
-53.401499	-19.355799	1.096051
-54.086775	-19.248785	1.101056
-54.232456	-12.133092	1.106061
-54.191303	-18.882710	1.111066
-54.071612	-13.373244	1.116070
-54.593326	-23.484341	1.121075
-55.443492	-13.690806	1.126080
-55.611549	-18.656427	1.131085
-55.840406	-22.516587	1.136090
-55.587308	-14.756343	1.141094
-55.878780	-19.231875	1.146099
-55.929818	-13.080629	1.151104
-56.838889	-15.899101	1.156109
-56.866820	-16.017374	1.161114
-57.489477	-16.877396	1.166118
-57.448439	-16.109032	1.171123
-57.474853	-15.651544	1.176128
-57.794799	-18.175283	1.181133
-57.440722	-19.709928	1.186138
-58.404259	-13.442689	1.191142
-59.028100	-12.820549	1.196147
-58.883752	-22.640775	1.201152
-59.336593	-17.966718	1.206157
-59.412652	-21.804626	1.211162
-59.330815	-14.832383	1.216166
-59.069061	-22.750629	1.221171
-59.616979	-24.110240	1.226176
-60.505328	-11.352766	1.231181
-60.459069	-18.496118	1.236186
-60.926161	-12.021214	1.241190
-61.142120	-17.210767	1.246195
-61.139827	-13.622819	1.251200
-61.288905	-21.149402	1.256205
-61.558124	-22.603121	1.261210
-62.313707	-9.805276	1.266214
-62.921273	-15.938343	1.271219
-62.638161	-17.584371	1.276224
-62.905660	-19.084353	1.281229
-62.838394	-27.400175	1.286234
-62.707141	-14.829321	1.291238
-62.993134	-15.451861	1.296243
-63.285571	-14.933149	1.301248
-64.354881	-16.643108	1.306253
-64.402933	-17.247236	1.311258
-65.049290	-10.258389	1.316262
-64.990684	-16.631429	1.321267
-65.148901	-20.524401	1.326272
-65.310932	-17.043426	1.331277
-65.157414	-14.260774	1.336282
-65.401198	-4.744269	1.341286
-66.058305	-13.075702	1.346291
-66.415777	-14.280375	1.351296
-67.068087	-11.033144	1.356301
-66.666837	-19.567477	1.361306
-67.008045	-13.479866	1.366310
-67.488825	-10.508695	1.371315
-66.875744	-21.626851	1.376320
-67.537035	-18.820159	1.381325
-68.037271	-17.979915	1.386330
-68.888445	-11.347866	1.391334
-68.803403	-20.415512	1.396339
-68.830369	-20.714898	1.401344
-68.792232	-6.933179	1.406349
-68.713436	-20.267890	1.411354
-69.785918	-10.093386	1.416358
-70.283562	-18.280730	1.421363
-70.065859	-11.529307	1.426368
-70.560907	-9.278403	1.431373
-70.222295	-19.035688	1.436378
-70.602789	-3.547173	1.441382
-71.029734	-15.709054	1.446387
-71.592307	-18.117032	1.451392
-72.088975	-15.320829	1.456397
-71.946771	-15.841618	1.461402
-72.162815	-6.191378	1.466406
-72.002648	-15.089528	1.471411
-72.022959	-10.464013	1.476416
-73.115265	-10.136653	1.481421
-73.189017	-17.779705	1.486426
-73.527186	-8.933498	1.491430
-73.778661	-15.206837	1.496435
-73.789308	-22.668531	1.501440
-74.094330	-4.969374	1.506445
-73.725682	-9.793200	1.511450
-74.693773	-6.383757	1.516454
-75.142483	-16.206209	1.521459
-75.118476	-10.075877	1.526464
-75.293676	-6.743283	1.531469
-75.198256	-16.212839	1.536474
-75.411729	-13.325404	1.541478
-75.771471	-13.614671	1.546483
-76.155916	-17.027561	1.551488
-76.344066	-14.507608	1.556493
-76.482343	-24.967741	1.561498
-77.529496	-8.711707	1.566502
-77.980936	-14.387559	1.571507
-77.943650	-19.116644	1.576512
-78.285471	-9.510695	1.581517
-77.916887	-23.831315	1.586522
-78.106904	-14.329443	1.591526
-78.048386	-8.760909	1.596531
-77.916222	-19.303721	1.601536
-79.027584	-6.968302	1.606541
-79.402440	-19.151435	1.611546
-79.593111	-15.679529	1.616550
-79.628474	-12.194667	1.621555
-80.009947	-17.223410	1.626560
-80.804878	-7.588003	1.631565
-80.941777	-11.508187	1.636570
-81.314669	-8.141274	1.641574
-81.135465	-19.712281	1.646579
-81.238695	-27.709196	1.651584
-81.294673	-22.684100	1.656589
-81.074902	-27.390125	1.661594
-82.252122	-11.667451	1.666598
-82.793088	-13.549563	1.671603
-82.727362	-13.157062	1.676608
-83.289857	-24.883270	1.681613
-82.816925	-30.009112	1.686618
-83.466691	-21.899845	1.691622
-83.404923	-16.467616	1.696627
-83.568291	-24.663744	1.701632
-84.460490	-18.016219	1.706637
-84.571428	-25.825971	1.711642
-85.001645	-19.883460	1.716646
-85.061452	-11.929121	1.721651
-84.699102	-21.615350	1.726656
-85.242659	-15.727671	1.731661
-84.960577	-16.827709	1.736666
-85.811741	-21.893903	1.741670
-86.424462	-17.850482	1.746675
-86.540281	-26.563798	1.751680
-86.393332	-18.008887	1.756685
-86.352717	-35.448674	1.761690
-87.249348	-17.273464	1.766694
-87.905997	-22.018056	1.771699
-87.844637	-22.996291	1.776704
-88.316731	-15.852984	1.781709
-87.960359	-18.726909	1.786714
-87.980127	-21.306673	1.791718
-87.973509	-8.948423	1.796723
-88.969712	-24.762958	1.801728
-89.283474	-9.425410	1.806733
-89.237397	-19.815240	1.811738
-89.126444	-11.642319	1.816742
-89.394892	-10.363705	1.821747
-90.154240	-10.831480	1.826752
-91.042328	-9.403475	1.831757
-91.160758	-22.456880	1.836762
-91.351795	-4.043117	1.841766
-91.281933	-11.199458	1.846771
-90.913038	-13.581338	1.851776
-91.451634	-6.240337	1.856781
-91.223414	-13.549985	1.861786
-91.858583	-14.417401	1.866790
-92.538989	-20.813872	1.871795
-92.733559	-17.160762	1.876800
-93.052488	-10.266989	1.881805
-92.785148	-17.466096	1.886810
-93.229287	-15.940924	1.891814
-93.688396	-16.636220	1.896819
-94.100646	-10.104685	1.901824
-94.442612	-10.767089	1.906829
-94.236312	-21.269884	1.911834
-94.173651	-11.769801	1.916838
-94.591385	-12.572391	1.921843
-95.123305	-19.160003	1.926848
-95.562495	-13.949487	1.931853
-95.461257	-26.183044	1.936858
-96.182361	-24.851761	1.941862
-96.045180	-18.112070	1.946867
-95.789104	-21.981500	1.951872
-96.569416	-20.335730	1.956877
-97.325175	-25.235387	1.961882
-97.627832	-15.525225	1.966886
-97.495698	-16.785132	1.971891
-97.586230	-21.655844	1.976896
-97.661799	-16.632042	1.981901
-97.616530	-24.523706	1.986906
-98.473799	-16.412234	1.991910
-99.163804	-19.398004	1.996915
-99.212933	-17.175109	2.006912
-98.224422	-17.469549	2.016909
-97.680711	-18.665205	2.026906
-97.516543	-18.941273	2.036902
-97.704719	-22.108532	2.046899
-96.684912	-13.224612	2.056896
-96.285679	-15.447688	2.066893
-95.367226	-27.852347	2.076890
-95.003461	-21.409016	2.086886
-94.950680	-13.076243	2.096883
-94.049236	-17.599791	2.106880
-93.414138	-21.052576	2.116877
-93.215692	-19.871404	2.126874
-92.333666	-15.100311	2.136870
-91.894015	-13.970348	2.146867
-91.917818	-19.394971	2.156864
-91.221937	-27.654190	2.166861
-90.242955	-18.874750	2.176858
-90.473246	-23.461596	2.186854
-89.499998	-24.850891	2.196851
-88.771360	-16.868933	2.206848
-88.579567	-15.508832	2.216845
-88.538604	-15.162652	2.226842
-87.538181	-17.745514	2.236838
-87.106406	-19.370357	2.246835
-85.886256	-23.326269	2.256832
-85.789861	-22.885143	2.266829
-85.777029	-19.558480	2.276826
-85.745050	-17.747499	2.286822
-84.728381	-17.746271	2.296819
-84.003865	-21.709406	2.306816
-83.010581	-22.067464	2.316813
-82.919875	-27.071819	2.326810
-82.859288	-23.206349	2.336806
-82.248404	-26.993583	2.346803
-81.877132	-16.534594	2.356800
-81.028478	-26.012329	2.366797
-80.127059	-29.426429	2.376794
-79.871474	-25.275736	2.386790
-79.970952	-20.910936	2.396787
-78.894264	-20.994728	2.406784
-77.925101	-26.641888	2.416781
-77.989780	-28.005696	2.426778
-78.063950	-22.663684	2.436774
-77.296828	-16.963087	2.446771
-76.848049	-14.257710	2.456768
-75.790258	-21.488967	2.466765
-75.195703	-19.999959	2.476762
-75.098480	-18.245821	2.486758
-74.643550	-21.652761	2.496755
-73.912281	-13.083220	2.506752
-73.366508	-21.440282	2.516749
-73.353970	-22.462213	2.526746
-72.400185	-16.912265	2.536742
-71.942645	-23.625033	2.546739
-71.865085	-23.728492	2.556736
-70.642526	-24.774967	2.566733
-70.391509	-29.986068	2.576730
-70.510429	-24.308852	2.586726
-69.484598	-20.463743	2.596723
-69.026992	-16.072650	2.606720
-68.652963	-21.576990	2.616717
-67.775878	-21.594331	2.626714
-67.378520	-19.595497	2.636710
-67.114338	-19.167734	2.646707
-66.673583	-21.849758	2.656704
-65.836423	-17.314257	2.666701
-65.787334	-17.441058	2.676698
-64.646707	-15.782858	2.686694
-64.626735	-16.237372	2.696691
-64.499279	-13.918009	2.706688
-63.282454	-16.427638	2.716685
-62.980804	-22.240276	2.726682
-62.636788	-14.543547	2.736678
-61.460414	-23.530221	2.746675
-61.375519	-18.112399	2.756672
-61.456782	-20.258861	2.766669
-60.565887	-17.801761	2.776666
-60.175192	-21.989587	2.786662
-59.559150	-13.003222	2.796659
-58.676188	-18.657247	2.806656
-58.468710	-14.470327	2.816653
-58.240033	-18.742167	2.826650
-57.150347	-7.931891	2.836646
-56.725632	-19.526290	2.846643
-56.703512	-17.798044	2.856640
-56.171694	-23.473937	2.866637
-55.101689	-20.555106	2.876634
-55.214269	-22.900881	2.886630
-54.692416	-19.227188	2.896627
-53.515772	-17.346542	2.906624
-53.386823	-15.678271	2.916621
-53.274166	-12.987961	2.926618
-52.672610	-19.746907	2.936614
-52.145264	-16.389270	2.946611
-51.504263	-18.955279	2.956608
-50.598268	-18.832180	2.966605
-50.185699	-20.952543	2.976602
-50.219574	-21.358820	2.986598
-49.457284	-20.616598	2.996595
-48.659853	-22.909764	3.006592
-48.415919	-25.334339	3.016589
-48.291798	-19.223365	3.026586
-47.296616	-23.098147	3.036582
-47.042722	-22.064267	3.046579
-46.748514	-23.912119	3.056576
-45.650106	-23.965120	3.066573
-45.446088	-20.588713	3.076570
-45.030300	-21.809807	3.086566
-43.922686	-21.406331	3.096563
-43.821192	-15.222255	3.106560
-44.028476	-21.189293	3.116557
-42.824048	-28.995098	3.126554
-42.263754	-21.788236	3.136550
-42.071572	-27.652490	3.146547
-41.804724	-26.407166	3.156544
-40.831281	-23.828981	3.166541
-40.695685	-27.420530	3.176538
-39.473512	-29.138326	3.186534
-39.276917	-29.212891	3.196531
-39.221661	-30.357484	3.206528
-38.464914	-24.020125	3.216525
-38.049877	-24.717296	3.226522
-37.540778	-25.304382	3.236518
-36.761730	-23.962892	3.246515
-36.432163	-23.712716	3.256512
-35.892438	-25.602610	3.266509
-35.471486	-26.938565	3.276506
-34.687221	-22.934298	3.286502
-34.439740	-25.266002	3.296499
-34.168568	-22.558871	3.306496
-33.345053	-26.207043	3.316493
-32.789827	-25.024491	3.326490
-32.729279	-18.513942	3.336486
-31.528579	-16.712750	3.346483
-31.340905	-16.688824	3.356480
-31.291156	-24.196121	3.366477
-30.575939	-27.476040	3.376474
-29.675891	-23.929585	3.386470
-29.557632	-22.027974	3.396467
-29.052288	-24.560844	3.406464
-28.383401	-25.430855	3.416461
-27.849250	-21.394650	3.426458
-26.826889	-18.295231	3.436454
-26.951167	-22.134394	3.446451
-26.504319	-16.937935	3.456448
-26.275144	-18.381034	3.466445
-25.272217	-23.241462	3.476442
-24.837297	-23.312420	3.486438
-24.652706	-19.245989	3.496435
-23.460529	-17.556402	3.506432
-23.332349	-20.764200	3.516429
-23.424216	-23.823528	3.526426
-22.148399	-19.958156	3.536422
-22.006613	-17.873722	3.546419
-21.395066	-23.292322	3.556416
-20.258301	-28.441454	3.566413
-20.650145	-23.791135	3.576410
-20.057356	-28.607550	3.586406
-19.610559	-17.230036	3.596403
-18.675624	-22.956283	3.606400
-18.267402	-24.449184	3.616397
-18.186619	-25.880748	3.626394
-17.204614	-22.635347	3.636390
-16.973935	-28.257811	3.646387
-16.359414	-25.361148	3.656384
-15.384826	-21.416253	3.666381
-15.098303	-22.412031	3.676378
-15.266912	-22.104252	3.686374
-14.932492	-28.504201	3.696371
-14.113233	-16.606872	3.706368
-13.046934	-14.386470	3.716365
-12.512552	-18.942676	3.726362
-12.389990	-22.582058	3.736358
-12.177079	-23.341387	3.746355
-11.281779	-22.046607	3.756352
-11.037340	-28.995168	3.766349
-10.232214	-28.598100	3.776346
-9.523265	-20.008648	3.786342
-9.384354	-18.989313	3.796339
-9.146429	-23.100268	3.806336
-8.536354	-28.777260	3.816333
-7.917103	-21.807376	3.826330
-7.410732	-23.559955	3.836326
-6.354948	-18.137724	3.846323
-6.376985	-20.821548	3.856320
-6.367492	-13.064275	3.866317
-5.465012	-2.771076	3.876314
-5.214446	-2.357651	3.886310
-4.491324	12.618984	3.896307
-4.188007	13.392567	3.906304
-3.671659	20.210773	3.916301
-3.133098	33.037438	3.926298
-2.589492	48.777274	3.936294
-2.484525	56.134664	3.946291
-1.782264	66.271581	3.956288
-1.118651	89.549452	3.966285
-0.776114	97.122210	3.976282
0.047443	108.371636	3.986278
0.000000	120.319201	3.991283
0.322190	129.584398	3.996288
0.713495	133.802778	4.001293
1.061518	136.513193	4.006298
0.899137	138.195362	4.011302
0.773965	141.640076	4.016307
0.702309	147.699293	4.021312
0.946785	140.542181	4.026317
0.717481	150.979122	4.031322
1.176222	136.720972	4.036326
0.897746	147.225845	4.041331
0.701374	140.989484	4.046336
0.826919	142.481893	4.051341
0.663303	151.465640	4.056346
1.027469	146.967323	4.061350
0.921793	147.708487	4.066355
0.714540	150.611497	4.071360
0.993281	154.790506	4.076365
1.165960	156.105995	4.081370
1.226319	149.985379	4.086374
0.941273	150.958513	4.091379
0.789224	144.651664	4.096384
1.137985	149.758980	4.101389
1.280061	159.109276	4.106394
1.110572	158.142420	4.111398
0.885534	162.114971	4.116403
1.413877	153.891809	4.121408
1.162450	159.830629	4.126413
0.944511	159.436568	4.131418
1.388217	165.723225	4.136422
1.306799	167.086121	4.141427
1.146368	153.034681	4.146432
1.449071	159.563529	4.151437
1.126717	159.240039	4.156442
1.286361	146.124840	4.161446
1.197644	147.684896	4.166451
1.425739	152.569868	4.171456
1.340094	156.822638	4.176461
1.009617	151.237582	4.181466
1.444877	160.418362	4.186470
0.839306	168.164806	4.191475
1.845768	168.679773	4.196480
1.875946	163.883134	4.201485
1.257914	151.212841	4.206490
1.288150	145.688823	4.211494
1.490302	146.755723	4.216499
1.236092	144.133054	4.221504
0.869018	153.426565	4.226509
1.400941	161.821143	4.231514
1.630538	159.000546	4.236518
1.364877	171.492250	4.241523
1.626003	164.985547	4.246528
1.605443	180.518248	4.251533
1.510637	173.094662	4.256538
2.017990	173.038115	4.261542
1.401795	157.583711	4.266547
1.041489	150.232715	4.271552
1.261350	170.468922	4.276557
1.488795	170.908649	4.281562
1.899362	172.141925	4.286566
1.716038	178.399023	4.291571
1.672192	175.864256	4.296576
1.774743	178.013851	4.301581
1.556335	163.953057	4.306586
1.283393	159.684560	4.311590
1.549898	178.890269	4.316595
1.748320	168.996040	4.321600
1.927664	177.784876	4.326605
1.305910	171.712677	4.331610
1.640716	171.771136	4.336614
1.627307	178.385689	4.341619
1.798236	167.340619	4.346624
1.784217	179.032892	4.351629
1.587322	171.031248	4.356634
1.627577	167.578170	4.361638
1.619839	171.990710	4.366643
1.889975	179.945968	4.371648
1.685465	175.815516	4.376653
1.690226	176.304749	4.381658
1.754244	169.431674	4.386662
1.586050	178.001791	4.391667
1.517284	163.389137	4.396672
1.790853	170.615854	4.401677
1.706879	182.559278	4.406682
1.781498	175.277146	4.411686
1.525997	174.929561	4.416691
1.920759	181.900991	4.421696
1.819466	187.499815	4.426701
1.696461	202.676737	4.431706
2.243595	207.515211	4.436710
2.511482	200.670325	4.441715
2.115004	188.382847	4.446720
1.800582	184.025504	4.451725
1.702409	183.620884	4.456730
1.707069	179.151701	4.461734
1.847383	203.950482	4.466739
2.204214	202.264995	4.471744
2.330404	203.099980	4.476749
1.972908	207.781400	4.481754
2.275791	197.108536	4.486758
1.881018	192.460600	4.491763
2.109709	200.917254	4.496768
2.282515	192.778206	4.501773
1.743571	198.284141	4.506778
2.088948	195.423448	4.511782
1.979789	205.273192	4.516787
2.163280	208.419152	4.521792
2.267759	203.494954	4.526797
1.924265	207.727091	4.531802
2.467989	207.511586	4.536806
2.096245	203.750013	4.541811
1.958484	204.544839	4.546816
2.141045	209.738701	4.551821
1.956620	214.469213	4.556826
2.285603	198.752874	4.561830
2.472202	209.010475	4.566835
2.243666	200.071187	4.571840
2.486436	206.363509	4.576845
2.414527	208.971597	4.581850
2.611363	203.079568	4.586854
2.238512	209.300772	4.591859
2.288689	199.759241	4.596864
1.955660	210.177483	4.601869
2.013628	207.998222	4.606874
2.504613	207.506104	4.611878
2.249122	210.016522	4.616883
2.278865	210.669749	4.621888
2.380464	204.678838	4.626893
2.202048	214.681349	4.631898
2.167056	207.037087	4.636902
1.995813	209.045347	4.641907
2.196078	223.514788	4.646912
2.484460	225.869039	4.651917
2.704923	227.625165	4.656922
2.590024	226.684589	4.661926
2.370241	237.067125	4.666931
2.729073	232.990781	4.671936
2.906109	226.111990	4.676941
2.403801	219.871004	4.681946
2.436604	216.845591	4.686950
2.360631	224.333471	4.691955
2.721921	223.561498	4.696960
3.077452	229.918235	4.701965
2.541264	230.603609	4.706970
2.388352	211.226958	4.711974
2.325006	236.002683	4.716979
2.653355	232.428277	4.721984
2.731473	241.249699	4.726989
2.558304	243.621182	4.731994
2.867834	236.615266	4.736998
2.520651	250.586735	4.742003
2.874303	234.551524	4.747008
2.604200	234.602605	4.752013
2.484971	236.389725	4.757018
2.881971	239.334179	4.762022
2.874277	246.554819	4.767027
2.806617	238.891679	4.772032
2.871625	245.852820	4.777037
2.660832	244.212189	4.782042
3.050045	241.705155	4.787046
2.952740	245.733141	4.792051
2.805864	244.684588	4.797056
3.010843	244.344418	4.802061
2.885221	239.524222	4.807066
3.001236	232.775709	4.812070
2.860971	240.239118	4.817075
2.564083	239.663556	4.822080
2.847401	243.940696	4.827085
2.781572	243.085727	4.832090
2.963525	238.341091	4.837094
2.511556	234.415784	4.842099
2.683935	236.189741	4.847104
2.789199	236.145511	4.852109
2.648301	242.652540	4.857114
3.014639	241.579583	4.862118
2.651355	243.846979	4.867123
2.741028	238.035040	4.872128
3.089076	247.105796	4.877133
2.873623	271.372775	4.882138
3.016552	267.292905	4.887142
3.061817	263.596056	4.892147
3.088472	267.011315	4.897152
2.818571	265.797439	4.902157
2.886474	265.497926	4.907162
3.077843	268.528929	4.912166
2.918000	274.347446	4.917171
2.981620	263.926096	4.922176
3.095612	270.146429	4.927181
3.086916	269.939520	4.932186
3.208037	266.636227	4.937190
3.005692	271.043132	4.942195
3.419396	268.807718	4.947200
2.987865	267.457410	4.952205
2.625281	280.803337	4.957210
3.003391	270.201242	4.962214
3.146819	296.991763	4.967219
3.446555	288.535050	4.972224
3.611517	298.991657	4.977229
3.513615	290.506660	4.982234
3.481459	271.536577	4.987238
3.087231	278.838606	4.992243
3.184294	260.552417	4.997248
3.818996	274.562793	5.002253
3.462107	273.528492	5.007258
3.428586	262.058404	5.012262
3.316242	272.259581	5.017267
3.509008	269.341463	5.022272
3.459874	261.720236	5.027277
3.363606	267.691223	5.032282
3.530738	266.555149	5.037286
3.435152	273.089419	5.042291
3.403974	268.292647	5.047296
3.634158	274.809281	5.052301
3.371216	271.675751	5.057306
3.450127	256.933571	5.062310
3.286287	272.641447	5.067315
3.436866	275.181130	5.072320
3.728298	283.458914	5.077325
3.247197	289.167438	5.082330
3.605547	285.185881	5.087334
3.665623	300.578857	5.092339
3.828505	294.381217	5.097344
3.661536	276.813819	5.102349
3.199810	283.835562	5.107354
3.644103	287.964302	5.112358
3.671231	303.123762	5.117363
3.670394	304.746045	5.122368
3.907709	300.779199	5.127373
3.687701	300.638265	5.132378
4.159674	293.819139	5.137382
3.671774	285.868386	5.142387
3.495789	271.098545	5.147392
3.324425	279.039544	5.152397
3.266801	290.991318	5.157402
3.689587	291.927366	5.162406
3.653835	310.033215	5.167411
3.791571	299.125763	5.172416
3.905611	296.969370	5.177421
3.924564	302.790851	5.182426
3.973310	291.903073	5.187430
3.992418	299.086542	5.192435
3.984607	292.429352	5.197440
3.962585	291.009059	5.202445
3.883668	297.525581	5.207450
4.020467	295.707206	5.212454
3.959959	305.318469	5.217459
3.917886	296.263394	5.222464
3.812831	296.699182	5.227469
3.592171	291.157656	5.232474
3.860716	296.417033	5.237478
3.787661	309.386869	5.242483
3.422900	291.206918	5.247488
3.536584	297.894803	5.252493
3.942086	302.337223	5.257498
4.137055	294.164852	5.262502
3.963203	296.929353	5.267507
4.045414	299.868522	5.272512
3.682927	295.814519	5.277517
3.616285	301.303256	5.282522
4.152132	305.044466	5.287526
4.257267	326.281821	5.292531
4.186658	311.904162	5.297536
4.181530	315.557354	5.302541
3.978492	310.469343	5.307546
4.153193	312.560241	5.312550
3.992414	322.352302	5.317555
3.804652	325.426760	5.322560
4.508416	327.766903	5.327565
4.436665	328.537386	5.332570
4.628906	318.748674	5.337574
4.326433	309.698034	5.342579
4.162198	298.848678	5.347584
3.993411	296.493831	5.352589
3.867218	297.968938	5.357594
4.068158	306.306909	5.362598
4.160908	324.906347	5.367603
4.650829	329.868789	5.372608
4.424412	329.854225	5.377613
4.254092	327.585073	5.382618
4.655296	327.680491	5.387622
4.337951	307.939431	5.392627
4.166290	304.826695	5.397632
4.292239	320.406513	5.402637
4.053190	321.960499	5.407642
4.418226	319.670580	5.412646
4.219854	330.194676	5.417651
4.028232	328.895213	5.422656
4.439328	323.905204	5.427661
4.357012	333.654679	5.432666
4.469615	326.966089	5.437670
4.311653	335.683589	5.442675
4.438319	328.771849	5.447680
4.408738	325.707412	5.452685
4.363594	332.168035	5.457690
4.748452	323.486451	5.462694
4.346822	327.621291	5.467699
4.056496	324.765399	5.472704
4.167728	324.627038	5.477709
4.092468	331.032855	5.482714
4.551603	336.637005	5.487718
4.557751	354.192699	5.492723
4.549968	348.770416	5.497728
4.562511	359.511802	5.502733
4.627495	355.650046	5.507738
5.059495	340.074571	5.512742
4.774803	357.112665	5.517747
4.739941	339.687307	5.522752
4.970278	332.556523	5.527757
4.407043	325.335545	5.532762
4.650488	326.458175	5.537766
4.256554	335.225999	5.542771
4.538763	346.938610	5.547776
4.842786	351.157098	5.552781
4.811891	361.265911	5.557786
5.044215	350.485237	5.562790
4.575194	363.123844	5.567795
4.760180	360.175226	5.572800
4.648611	360.258072	5.577805
4.866224	358.029462	5.582810
5.075745	345.381023	5.587814
4.589103	359.160784	5.592819
4.720065	356.922843	5.597824
5.198967	362.609572	5.602829
4.938630	360.635935	5.607834
4.992468	358.007606	5.612838
4.726153	356.467523	5.617843
4.785155	352.723385	5.622848
4.719797	355.626418	5.627853
4.750769	361.128613	5.632858
4.988207	350.586659	5.637862
4.686656	359.624942	5.642867
5.006272	362.900737	5.647872
5.132199	358.388135	5.652877
4.766181	363.513245	5.657882
5.409272	353.640183	5.662886
5.293205	355.425609	5.667891
5.164954	351.391609	5.672896
5.083154	351.733167	5.677901
5.205012	361.692166	5.682906
5.069894	350.810325	5.687910
5.186401	362.167554	5.692915
5.030396	356.738239	5.697920
5.263439	345.508705	5.702925
4.810506	356.132791	5.707930
5.283632	355.877077	5.712934
5.122290	350.866016	5.717939
5.357752	359.292626	5.722944
5.398434	359.666000	5.727949
4.971442	361.015491	5.732954
5.076480	355.886315	5.737958
5.047063	361.518096	5.742963
5.393602	358.825510	5.747968
5.277094	357.124851	5.752973
4.967743	357.215585	5.757978
5.385212	354.073165	5.762982
5.237895	354.647775	5.767987
5.022921	352.627949	5.772992
5.170723	358.419431	5.777997
4.984678	360.807075	5.783002
5.240826	350.031929	5.788006
5.410800	356.730843	5.793011
5.061783	361.014849	5.798016
5.299990	353.142146	5.803021
5.230163	352.913589	5.808026
5.222849	354.766650	5.813030
4.977167	369.882550	5.818035
5.470462	377.723797	5.823040
5.373621	379.769684	5.828045
5.356758	386.507445	5.833050
5.293911	381.133144	5.838054
5.575962	391.810189	5.843059
5.417373	393.808878	5.848064
5.453535	379.625613	5.853069
5.573586	392.961769	5.858074
5.819713	381.716821	5.863078
5.487973	401.991195	5.868083
5.589601	391.166027	5.873088
5.637747	393.967391	5.878093
5.498299	391.565046	5.883098
5.939629	384.537632	5.888102
5.508783	371.279076	5.893107
5.351128	361.000865	5.898112
5.531205	381.145662	5.903117
5.466139	386.801115	5.908122
5.513396	378.808859	5.913126
5.508158	394.129665	5.918131
5.666353	392.799106	5.923136
5.400528	388.916148	5.928141
5.368970	390.764150	5.933146
5.692135	391.859574	5.938150
5.415589	393.039703	5.943155
5.133180	395.437587	5.948160
5.502035	386.086290	5.953165
5.303874	395.011172	5.958170
5.770453	407.232030	5.963174
5.763921	420.360851	5.968179
6.184411	418.714529	5.973184
5.912286	416.069915	5.978189
5.783213	407.849121	5.983194
5.741826	392.643452	5.988198
5.390330	409.307659	5.993203
5.648644	417.612707	5.998208
5.691363	420.010628	6.003213
5.889010	423.438456	6.008218
5.762165	419.509781	6.013222
5.724944	421.312548	6.018227
6.069608	421.781023	6.023232
6.401397	422.909555	6.028237
5.868415	419.360717	6.033242
5.989737	417.034576	6.038246
5.793670	404.255914	6.043251
5.827133	404.385982	6.048256
5.910664	398.938299	6.053261
5.911467	405.425878	6.058266
5.678143	387.439739	6.063270
5.990037	400.822081	6.068275
5.367133	401.259954	6.073280
5.807181	407.677561	6.078285
5.711514	422.000828	6.083290
6.087377	413.854483	6.088294
6.045163	417.150739	6.093299
5.867527	410.311259	6.098304
5.785737	411.276010	6.103309
5.918664	419.479275	6.108314
5.917026	412.092243	6.113318
5.732414	409.113057	6.118323
5.792371	400.089176	6.123328
6.089652	407.818841	6.128333
5.785783	404.711993	6.133338
5.845969	397.896284	6.138342
5.809243	400.545742	6.143347
5.629701	394.678078	6.148352
5.877290	407.095043	6.153357
5.486208	411.218291	6.158362
6.132000	411.952444	6.163366
6.155958	421.692664	6.168371
5.887618	403.729670	6.173376
5.735656	393.449902	6.178381
5.860587	394.280567	6.183386
5.978549	390.974613	6.188390
5.761627	387.752531	6.193395
5.558224	394.397059	6.198400
5.738607	393.311471	6.203405
5.749924	406.550202	6.208410
6.022020	405.476462	6.213414
5.963880	406.707452	6.218419
5.571035	393.054815	6.223424
5.430111	402.791147	6.228429
5.772316	409.221009	6.233434
6.291836	415.028314	6.238438
5.597754	415.330563	6.243443
5.688314	420.637611	6.248448
6.312488	417.709201	6.253453
5.751422	415.182292	6.258458
6.010032	408.664459	6.263462
5.909938	399.024945	6.268467
5.678596	396.246101	6.273472
5.787826	391.155292	6.278477
5.756832	400.136166	6.283482
5.940479	408.481990	6.288486
5.989718	408.988137	6.293491
5.519137	401.624497	6.298496
6.020293	406.182929	6.303501
5.722307	412.053185	6.308506
6.213255	413.550036	6.313510
5.737733	406.322980	6.318515
5.672850	397.644591	6.323520
5.901544	379.906967	6.328525
5.625920	397.899506	6.333530
5.830665	402.711858	6.338534
5.789418	413.169734	6.343539
5.899162	418.481892	6.348544
6.157816	424.357461	6.353549
6.040306	409.160237	6.358554
5.820783	394.862809	6.363558
5.789388	395.184774	6.368563
5.608281	391.368497	6.373568
5.355123	386.823347	6.378573
5.965286	408.315421	6.383578
6.140410	417.117919	6.388582
5.972460	411.574923	6.393587
6.007112	391.692783	6.398592
6.092063	391.761044	6.403597
5.832453	386.448136	6.408602
6.097465	394.830405	6.413606
5.818258	390.457502	6.418611
5.782508	398.976209	6.423616
6.172964	383.413885	6.428621
5.475850	396.618364	6.433626
5.598616	387.630069	6.438630
5.682713	394.741843	6.443635
5.537321	396.872142	6.448640
5.730862	392.143695	6.453645
5.666474	399.008917	6.458650
5.979469	407.207616	6.463654
5.674754	410.495243	6.468659
5.890318	417.124867	6.473664
5.911027	418.049754	6.478669
5.966398	415.655204	6.483674
5.949389	404.083805	6.488678
6.104777	397.103144	6.493683
5.584180	398.433013	6.498688
5.771639	389.821377	6.503693
5.609298	392.712061	6.508698
5.806981	401.835830	6.513702
5.855782	410.353763	6.518707
5.685516	408.959587	6.523712
6.273265	420.966408	6.528717
5.745074	409.521292	6.533722
5.554814	396.251291	6.538726
5.725071	407.954071	6.543731
5.575518	417.665793	6.548736
6.165271	419.288366	6.553741
5.927218	434.024571	6.558746
6.112335	422.892903	6.563750
5.936723	401.805300	6.568755
5.826285	400.171713	6.573760
5.954847	393.265157	6.578765
5.636958	392.871854	6.583770
5.900050	396.175171	6.588774
5.578428	395.370050	6.593779
5.510137	392.493165	6.598784
5.619908	409.584595	6.603789
5.987902	430.292917	6.608794
5.982155	422.743165	6.613798
5.803576	435.861022	6.618803
5.964757	425.854788	6.623808
5.934980	421.488131	6.628813
5.854079	419.189950	6.633818
6.175686	406.673864	6.638822
5.938141	395.722518	6.643827
5.911113	391.344955	6.648832
5.833874	395.317954	6.653837
6.039755	396.811885	6.658842
5.924788	389.581767	6.663846
5.657881	389.254220	6.668851
5.769419	389.931206	6.673856
5.995663	394.116409	6.678861
5.678280	395.513268	6.683866
5.756514	393.618738	6.688870
5.876423	403.974736	6.693875
5.630033	387.258260	6.698880
5.738701	393.561617	6.703885
5.712861	398.885367	6.708890
5.851724	388.190790	6.713894
5.796367	397.663318	6.718899
5.688752	400.698272	6.723904
6.271379	393.951554	6.728909
5.630701	400.234352	6.733914
5.489826	388.172767	6.738918
5.733779	405.457860	6.743923
6.099272	410.787853	6.748928
6.097172	403.462471	6.753933
5.811099	400.866939	6.758938
6.038408	393.536133	6.763942
5.914975	386.993561	6.768947
5.520086	394.327919	6.773952
5.892984	396.743781	6.778957
5.513452	396.146377	6.783962
5.855552	396.344923	6.788966
5.946108	399.422444	6.793971
5.685490	401.387511	6.798976
6.125794	401.346804	6.803981
5.499758	403.016188	6.808986
5.933046	398.271127	6.813990
5.624761	406.967776	6.818995
5.835253	414.254782	6.824000
6.156530	420.767445	6.829005
5.528913	410.136630	6.834010
6.061848	410.312061	6.839014
5.806700	406.864630	6.844019
5.461443	407.046559	6.849024
6.136699	410.101458	6.854029
5.725292	430.004647	6.859034
5.950787	421.267899	6.864038
6.044578	423.914889	6.869043
5.864986	408.538502	6.874048
5.883862	401.378766	6.879053
5.724312	403.236519	6.884058
6.004888	394.424951	6.889062
5.969472	394.130902	6.894067
5.461874	391.417736	6.899072
5.845907	393.893521	6.904077
5.450419	397.983553	6.909082
5.960093	403.054047	6.914086
5.851329	417.094326	6.919091
6.005450	415.547565	6.924096
5.847116	403.742635	6.929101
5.689483	404.931096	6.934106
5.951187	416.407588	6.939110
5.685803	414.093386	6.944115
5.925083	423.764009	6.949120
5.780724	417.299878	6.954125
5.846016	424.153701	6.959130
6.194709	420.115297	6.964134
6.041897	410.484506	6.969139
5.857535	402.335426	6.974144
5.939188	391.426540	6.979149
5.550014	403.201037	6.984154
5.877832	391.497558	6.989158
5.919808	392.465099	6.994163
5.849790	404.346195	6.999168
5.500504	395.298915	7.004173
5.801183	397.239313	7.009178
5.821405	398.901335	7.014182
5.698023	402.505457	7.019187
5.815876	404.795818	7.024192
5.986481	405.747782	7.029197
5.875908	409.111597	7.034202
5.954466	405.766580	7.039206
5.774232	402.864224	7.044211
5.826515	389.174782	7.049216
6.038202	394.650614	7.054221
5.946894	398.853869	7.059226
6.039052	390.877457	7.064230
5.859151	406.318171	7.069235
5.916647	396.550736	7.074240
5.761434	387.044285	7.079245
5.845407	401.054410	7.084250
6.124174	399.137131	7.089254
6.189261	393.521215	7.094259
5.347065	399.084738	7.099264
5.745378	398.134154	7.104269
5.822373	399.394073	7.109274
6.026861	398.846382	7.114278
6.328654	399.738733	7.119283
5.815510	397.761370	7.124288
5.542283	391.356873	7.129293
5.484638	402.380263	7.134298
5.763837	395.015605	7.139302
5.550584	401.888706	7.144307
5.594977	402.388946	7.149312
5.753209	406.433859	7.154317
5.661297	403.248301	7.159322
5.936996	406.297927	7.164326
6.022971	400.981463	7.169331
5.948420	398.645134	7.174336
6.147696	392.575223	7.179341
5.591723	409.806892	7.184346
6.013926	399.813496	7.189350
5.692631	410.012462	7.194355
5.698218	404.459677	7.199360
5.647119	404.286626	7.204365
5.697473	413.327447	7.209370
5.951707	401.938071	7.214374
5.753334	411.502766	7.219379
5.476883	410.302791	7.224384
5.884212	411.984580	7.229389
5.875499	430.014458	7.234394
5.994894	420.384170	7.239398
5.759568	420.127170	7.244403
6.141396	417.319406	7.249408
5.898073	406.497279	7.254413
5.868460	408.911518	7.259418
5.973213	403.256074	7.264422
5.862103	404.238507	7.269427
5.595452	403.524925	7.274432
6.109760	397.101509	7.279437
5.593022	403.764776	7.284442
5.967284	395.486292	7.289446
5.932451	397.504153	7.294451
5.756581	404.281868	7.299456
5.497648	403.694882	7.304461
6.034795	398.765477	7.309466
5.776566	401.584226	7.314470
5.968946	405.324518	7.319475
5.558383	407.655810	7.324480
5.827268	400.264835	7.329485
5.867703	411.234694	7.334490
5.828094	399.403595	7.339494
5.606708	400.070590	7.344499
5.749491	420.175437	7.349504
6.389811	411.951753	7.354509
5.742800	410.576926	7.359514
6.045998	400.076147	7.364518
5.834091	400.435897	7.369523
5.853167	404.475239	7.374528
6.019180	399.925203	7.379533
5.719248	401.715624	7.384538
6.073179	403.478283	7.389542
6.070570	402.356297	7.394547
5.963327	412.814643	7.399552
6.299506	400.262403	7.404557
5.769299	403.372468	7.409562
5.844102	407.954142	7.414566
5.972945	397.107295	7.419571
5.833940	408.088513	7.424576
6.115613	402.406733	7.429581
5.674449	411.488688	7.434586
6.081090	401.116019	7.439590
6.044579	410.148725	7.444595
5.646610	401.703490	7.449600
5.942986	404.093939	7.454605
5.615446	405.545367	7.459610
5.803423	402.859692	7.464614
5.811014	408.324531	7.469619
5.643262	413.025109	7.474624
5.790265	409.166533	7.479629
5.444911	405.661419	7.484634
5.454622	402.803979	7.489638
5.654355	411.695937	7.494643
5.911967	400.301464	7.499648
5.886411	401.679600	7.504653
5.790622	417.466340	7.509658
6.086479	406.267604	7.514662
5.937397	407.278821	7.519667
5.719082	406.805486	7.524672
5.884965	406.605582	7.529677
5.901496	412.583007	7.534682
5.870374	409.297395	7.539686
5.837994	412.709635	7.544691
5.582721	415.202881	7.549696
5.862138	398.243426	7.554701
5.783721	404.319650	7.559706
5.450322	408.899062	7.564710
5.763996	404.248203	7.569715
5.687081	411.883148	7.574720
5.879981	399.820353	7.579725
5.794764	403.102810	7.584730
5.915317	404.176531	7.589734
5.766366	402.114587	7.594739
5.705167	407.022089	7.599744
5.637779	399.902490	7.604749
5.812096	414.079611	7.609754
5.928594	411.075427	7.614758
5.762338	419.258180	7.619763
5.679598	429.330630	7.624768
6.181545	419.912280	7.629773
5.928182	420.787040	7.634778
5.791780	403.545373	7.639782
5.910034	408.741465	7.644787
5.464898	399.563630	7.649792
5.656587	412.656463	7.654797
5.738724	430.086388	7.659802
6.030918	433.063430	7.664806
5.978213	435.004334	7.669811
5.859355	420.891695	7.674816
5.827083	409.764659	7.679821
5.905072	409.199237	7.684826
5.989642	405.691999	7.689830
5.582167	408.137433	7.694835
5.596352	411.918483	7.699840
6.061873	420.312358	7.704845
5.944066	429.844976	7.709850
5.856427	415.391105	7.714854
5.944903	415.230660	7.719859
5.810366	406.983538	7.724864
5.759779	392.297207	7.729869
5.997079	402.733025	7.734874
5.882539	395.495335	7.739878
5.921241	401.104996	7.744883
5.713655	409.293798	7.749888
6.085593	399.107639	7.754893
5.774563	409.407323	7.759898
5.378697	407.042898	7.764902
5.744194	409.809079	7.769907
5.744777	410.239217	7.774912
5.884123	424.690124	7.779917
5.987358	426.446741	7.784922
5.632979	421.281139	7.789926
5.575692	420.901711	7.794931
5.939272	435.837455	7.799936
6.212075	423.788050	7.804941
5.685525	424.552546	7.809946
5.923597	420.080755	7.814950
6.009499	410.721438	7.819955
6.073353	405.696157	7.824960
5.815893	411.501881	7.829965
5.927008	399.720613	7.834970
5.814012	397.490899	7.839974
5.427689	403.988118	7.844979
5.427549	405.195098	7.849984
5.903539	419.130850	7.854989
6.013347	425.303591	7.859994
5.930747	422.704159	7.864998
5.721127	414.168920	7.870003
5.892417	422.388528	7.875008
5.767011	406.696112	7.880013
5.883602	430.066315	7.885018
5.723378	429.430028	7.890022
5.760223	431.464243	7.895027
5.782013	441.613522	7.900032
6.129437	436.942658	7.905037
5.891758	436.097981	7.910042
5.854678	411.169524	7.915046
5.923206	407.689018	7.920051
5.290593	409.741143	7.925056
5.987506	420.233671	7.930061
6.085818	431.685134	7.935066
5.654971	415.552509	7.940070
5.832019	419.200621	7.945075
6.096304	426.766838	7.950080
6.191148	409.928512	7.955085
5.940450	402.295010	7.960090
5.590427	394.043913	7.965094
6.041188	395.410464	7.970099
5.557393	405.511422	7.975104
5.801546	396.937953	7.980109
5.960602	406.123770	7.985114
5.974062	402.378479	7.990118
6.217828	403.851612	7.995136
5.848432	404.980450	8.000154
5.961045	406.782952	8.005171
5.695914	400.339828	8.010189
6.031224	401.539947	8.015206
6.076818	408.654884	8.020224
5.690881	408.715486	8.025242
5.653166	402.803357	8.030259
5.800322	413.450991	8.035277
5.598842	402.656538	8.040294
5.950542	412.800457	8.045312
5.561762	409.840122	8.050330
5.788628	402.002837	8.055347
5.754461	411.109562	8.060365
5.990149	411.255006	8.065382
6.201987	411.529389	8.070400
5.682699	410.016337	8.075418
5.993336	408.450887	8.080435
5.524750	408.825544	8.085453
5.733548	424.858012	8.090470
5.703221	423.046683	8.095488
6.113447	433.421259	8.100506
6.336890	431.726556	8.105523
5.944388	436.316426	8.110541
6.030629	435.058583	8.115558
5.976374	431.263973	8.120576
5.684595	433.011799	8.125594
5.780249	427.370072	8.130611
5.986564	433.464392	8.135629
5.959628	426.516102	8.140646
6.105431	435.389709	8.145664
5.629724	437.629767	8.150682
6.181509	429.174930	8.155699
6.098411	429.886114	8.160717
6.047758	433.062201	8.165734
6.695768	428.261805	8.170752
6.100787	424.487256	8.175770
6.150843	410.820860	8.180787
6.014868	408.481207	8.185805
6.075649	405.330492	8.190822
6.196330	407.974896	8.195840
5.785047	414.254347	8.200858
5.704839	403.897254	8.205875
6.153078	416.263785	8.210893
5.960191	431.005209	8.215910
6.397871	432.286009	8.220928
6.000818	424.971091	8.225946
5.988998	408.183503	8.230963
5.761463	420.934756	8.235981
6.018762	432.629235	8.240998
6.314911	436.763364	8.246016
6.141660	446.291534	8.251034
6.235707	437.349150	8.256051
6.240517	439.978104	8.261069
5.858086	428.352839	8.266086
6.218640	430.499491	8.271104
5.858686	444.407048	8.276122
6.161334	437.420317	8.281139
6.392194	439.146553	8.286157
6.327941	434.566653	8.291174
6.157283	425.507098	8.296192
5.817057	419.402557	8.301210
6.112170	420.326483	8.306227
6.072304	435.836799	8.311245
6.012798	428.208721	8.316262
6.236090	428.336337	8.321280
6.345942	437.190507	8.326298
6.251047	424.549794	8.331315
6.313976	432.802135	8.336333
6.265658	433.396348	8.341350
6.451000	431.117057	8.346368
5.880811	433.116875	8.351386
6.226606	432.133939	8.356403
6.481923	443.009136	8.361421
6.070116	427.138090	8.366438
6.175988	427.046193	8.371456
6.150838	434.599398	8.376474
6.335866	430.245915	8.381491
6.429782	442.852623	8.386509
5.956647	422.396040	8.391526
6.357128	418.219858	8.396544
6.086577	433.369585	8.401562
6.247972	433.595830	8.406579
6.009877	429.524996	8.411597
6.166082	430.604591	8.416614
6.383993	435.379184	8.421632
6.336011	436.101482	8.426650
6.462258	434.454367	8.431667
6.180167	446.695818	8.436685
6.016137	444.483236	8.441702
6.433595	423.187694	8.446720
5.784865	441.263996	8.451738
5.821364	436.028486	8.456755
6.080702	433.482040	8.461773
5.749681	436.372101	8.466790
6.016222	436.295131	8.471808
6.167742	457.537294	8.476826
6.639340	462.555296	8.481843
6.897128	445.787584	8.486861
6.350978	441.954555	8.491878
6.526186	430.810916	8.496896
6.429957	435.167881	8.501914
6.246383	426.877332	8.506931
6.196930	430.464604	8.511949
6.155736	421.538915	8.516966
6.481194	437.668014	8.521984
6.400801	442.885282	8.527002
6.420388	441.924673	8.532019
6.501989	433.040647	8.537037
6.210232	424.557007	8.542054
6.688638	434.873841	8.547072
6.317018	441.600241	8.552090
6.260853	437.830748	8.557107
6.601052	450.745077	8.562125
6.437934	446.831887	8.567143
6.459931	427.561513	8.572160
6.511243	435.253422	8.577178
6.532216	433.148188	8.582195
6.232640	429.818775	8.587213
6.142523	446.901865	8.592231
6.883621	446.048138	8.597248
6.606592	451.893199	8.602266
6.663506	444.087579	8.607283
6.620551	430.500540	8.612301
6.395038	427.438565	8.617319
6.437761	427.431332	8.622336
6.412247	436.491958	8.627354
6.456793	427.350115	8.632371
6.426223	430.367967	8.637389
6.199266	440.967344	8.642407
6.859624	446.456406	8.647424
6.652835	458.680869	8.652442
6.672113	455.639569	8.657459
6.414748	437.746244	8.662477
6.296487	439.156700	8.667495
6.928775	453.080846	8.672512
6.648146	446.216877	8.677530
6.468116	433.831574	8.682547
6.493952	427.545358	8.687565
6.645331	445.497045	8.692583
6.520217	430.206424	8.697600
6.648961	432.742616	8.702618
6.175932	444.308457	8.707635
6.780101	447.302298	8.712653
6.462362	464.800040	8.717671
6.952167	454.022957	8.722688
6.731545	457.572246	8.727706
6.516161	455.732901	8.732723
6.751695	443.048676	8.737741
6.307149	447.147404	8.742759
6.615465	455.791765	8.747776
6.798411	456.186279	8.752794
6.748872	459.267115	8.757811
6.665020	457.298124	8.762829
6.397090	474.211492	8.767847
6.890946	461.758469	8.772864
6.919622	465.189121	8.777882
6.575325	452.504455	8.782899
6.597978	442.118100	8.787917
6.646207	462.765612	8.792935
6.864594	453.437105	8.797952
7.064768	463.420535	8.802970
6.810932	444.002130	8.807987
6.910621	434.478938	8.813005
6.479456	439.014980	8.818023
6.817913	428.758213	8.823040
6.400640	431.364154	8.828058
6.648325	446.792419	8.833075
6.745665	449.750119	8.838093
7.083561	458.508866	8.843111
7.011657	448.314528	8.848128
6.595619	435.665376	8.853146
6.680198	429.279676	8.858163
6.616257	429.963674	8.863181
6.905145	439.046838	8.868199
7.191620	425.338327	8.873216
6.876309	432.465602	8.878234
6.510566	429.648878	8.883251
6.768961	417.059895	8.888269
6.429765	430.742761	8.893287
6.751433	447.197471	8.898304
6.828804	457.469321	8.903322
6.661127	459.506614	8.908339
6.787259	460.265627	8.913357
6.659905	465.257430	8.918375
6.691095	466.153808	8.923392
6.944595	463.531165	8.928410
6.981817	465.485714	8.933427
7.219222	457.614768	8.938445
6.879051	460.026662	8.943463
6.986991	455.529453	8.948480
6.807986	465.806364	8.953498
6.761556	457.803891	8.958515
6.898762	459.310814	8.963533
6.450127	463.867865	8.968551
6.695843	453.600457	8.973568
7.216377	459.040242	8.978586
6.853616	450.111886	8.983603
6.856681	444.549849	8.988621
6.762449	451.296850	8.993639
6.972378	448.728861	8.998656
7.081927	456.132616	9.003674
6.937117	465.265568	9.008691
7.405369	452.413280	9.013709
6.923108	464.579240	9.018727
6.715617	458.748152	9.023744
6.847932	453.962874	9.028762
6.651401	455.107378	9.033779
7.167077	444.327199	9.038797
6.984238	455.634184	9.043815
6.944319	453.698466	9.048832
7.044656	460.719921	9.053850
7.138966	453.929283	9.058867
7.278864	450.401708	9.063885
7.109059	455.343061	9.068903
7.174775	462.242897	9.073920
6.989949	453.935613	9.078938
7.030681	460.131963	9.083955
7.203317	452.887052	9.088973
6.812202	461.427177	9.093991
6.953957	458.590576	9.099008
7.158262	461.358927	9.104026
6.970328	461.584953	9.109043
7.075972	449.411366	9.114061
7.036712	462.409799	9.119079
7.214565	453.315743	9.124096
7.062792	445.276197	9.129114
7.060617	461.037561	9.134131
7.158177	449.323151	9.139149
6.934348	459.004772	9.144167
7.318144	446.015699	9.149184
7.232785	452.384293	9.154202
6.748435	462.935370	9.159219
6.813453	456.871179	9.164237
7.069878	450.454847	9.169255
7.036455	453.016125	9.174272
7.093377	457.943555	9.179290
7.135104	453.072302	9.184307
7.135303	448.029005	9.189325
7.015902	462.320136	9.194343
7.424475	466.918689	9.199360
7.137946	464.212847	9.204378
6.732617	459.555966	9.209395
7.271617	465.058242	9.214413
7.494645	478.972039	9.219431
7.031085	474.593870	9.224448
7.172252	487.306364	9.229466
7.011792	490.197715	9.234483
7.358201	484.782533	9.239501
7.145204	487.612117	9.244519
7.185858	482.455032	9.249536
7.150086	485.071030	9.254554
7.487884	489.517150	9.259571
7.456266	485.200117	9.264589
7.214952	479.948593	9.269607
7.251518	481.622763	9.274624
7.181050	478.494162	9.279642
7.028811	473.391657	9.284659
7.422198	481.560564	9.289677
7.166260	481.896466	9.294695
7.339841	486.923082	9.299712
7.552731	479.870493	9.304730
7.150935	481.647762	9.309747
7.415530	475.918400	9.314765
7.386579	490.823073	9.319783
7.355795	489.067518	9.324800
7.480769	487.758771	9.329818
7.083410	489.186908	9.334835
7.340640	488.243435	9.339853
7.403101	492.745976	9.344871
7.334848	492.951594	9.349888
7.527195	477.192246	9.354906
7.343315	488.802358	9.359923
7.737897	484.007890	9.364941
7.490959	485.684719	9.369959
7.331813	488.497710	9.374976
7.425002	494.239555	9.379994
7.363819	489.469381	9.385011
7.828869	479.240827	9.390029
7.451836	486.198440	9.395047
7.321217	493.905546	9.400064
7.899091	479.387768	9.405082
7.375904	489.510485	9.410099
7.361139	480.691598	9.415117
7.611567	482.405544	9.420135
7.135179	485.672808	9.425152
7.493734	488.940974	9.430170
7.302018	495.215788	9.435187
7.341750	485.719420	9.440205
7.330396	484.797591	9.445223
7.283057	490.916616	9.450240
7.616099	485.680799	9.455258
7.253268	492.470525	9.460275
7.624920	490.236154	9.465293
7.206011	489.900475	9.470311
7.099086	498.034925	9.475328
7.622375	491.018326	9.480346
7.425247	507.404297	9.485363
7.657867	512.519759	9.490381
7.790268	513.979456	9.495399
7.571578	506.951081	9.500416
7.503741	494.736703	9.505434
7.413693	505.979347	9.510451
7.892397	501.828966	9.515469
7.661674	504.747702	9.520487
7.569201	503.730652	9.525504
7.393413	497.024089	9.530522
7.662939	521.107212	9.535539
7.721685	515.942001	9.540557
7.685101	511.820848	9.545575
7.802816	525.015173	9.550592
7.740516	509.192261	9.555610
7.444779	501.954419	9.560627
7.522310	503.060827	9.565645
7.515664	517.311684	9.570663
7.885316	510.140807	9.575680
8.049726	505.163402	9.580698
7.538203	511.634083	9.585715
8.012622	514.933458	9.590733
7.924844	507.758217	9.595751
7.657535	495.368028	9.600768
7.991559	491.512256	9.605786
7.635326	484.480882	9.610803
7.644434	480.278752	9.615821
7.712017	483.711232	9.620839
7.433898	494.075042	9.625856
7.874304	494.417081	9.630874
7.612109	502.320572	9.635891
7.984850	517.874448	9.640909
8.065656	511.788134	9.645927
8.201569	501.235357	9.650944
7.714124	489.385721	9.655962
7.543098	482.794706	9.660979
7.530623	488.668015	9.665997
7.999709	498.453995	9.671015
7.755588	496.179280	9.676032
7.876838	497.964419	9.681050
7.702250	496.450179	9.686067
8.089552	500.138554	9.691085
7.946641	494.284161	9.696103
7.747936	489.160214	9.701120
8.138110	480.531732	9.706138
7.541696	487.206013	9.711155
7.520929	497.039844	9.716173
7.983794	511.152323	9.721191
8.071287	512.143310	9.726208
8.126626	511.503130	9.731226
8.047057	504.955027	9.736243
7.763912	495.847134	9.741261
7.758438	490.476048	9.746279
7.867207	501.928858	9.751296
8.107067	514.877571	9.756314
7.657611	515.893306	9.761331
7.918923	522.149604	9.766349
8.111155	519.312507	9.771367
7.479764	521.942110	9.776384
7.897245	513.364202	9.781402
8.012959	518.756093	9.786419
7.684095	518.372827	9.791437
7.954143	519.997314	9.796455
7.631138	522.845909	9.801472
7.902909	519.946432	9.806490
7.960233	512.794007	9.811507
7.929446	518.371760	9.816525
8.270444	514.466603	9.821543
7.662955	512.747099	9.826560
8.005944	513.790652	9.831578
7.636791	517.730271	9.836595
7.890037	518.362734	9.841613
8.135131	526.248763	9.846631
8.058016	535.739417	9.851648
8.515337	538.179093	9.856666
8.059807	527.684476	9.861683
7.823559	525.271062	9.866701
8.097684	529.958822	9.871719
8.131834	551.226849	9.876736
8.609728	539.065560	9.881754
7.958854	529.467793	9.886771
8.094287	526.014556	9.891789
8.075089	516.582846	9.896807
8.014523	536.688868	9.901824
8.383053	543.010485	9.906842
8.280528	547.981866	9.911859
8.067557	526.233729	9.916877
8.273193	516.470517	9.921895
8.046585	518.889596	9.926912
8.377004	522.408473	9.931930
8.363673	520.976968	9.936947
8.080288	513.823683	9.941965
8.311398	517.086583	9.946983
8.284682	520.637829	9.952000
8.138259	517.874921	9.957018
8.121723	512.694227	9.962035
8.092525	529.566351	9.967053
8.383196	535.634736	9.972071
8.226115	551.249217	9.977088
8.129989	544.295010	9.982106
8.284116	551.712687	9.987123
8.042584	554.119087	9.992141
8.439811	547.232582	9.997159
8.387791	557.258227	10.002176
8.289365	548.370681	10.007194
8.041196	553.823431	10.012211
8.386227	546.356635	10.017229
8.755864	537.937020	10.022247
8.496078	549.836694	10.027264
8.120830	546.121193	10.032282
8.185202	549.640434	10.037299
8.121091	546.438528	10.042317
8.434461	544.880485	10.047335
8.506868	547.058729	10.052352
8.417804	543.106679	10.057370
8.673702	548.008865	10.062387
8.264669	553.736857	10.067405
8.170083	551.141724	10.072423
8.206919	557.187195	10.077440
8.814625	544.635141	10.082458
8.432295	552.286917	10.087475
8.484843	553.327194	10.092493
8.382695	541.794199	10.097511
8.609573	547.646004	10.102528
8.485753	552.697284	10.107546
8.662642	557.812346	10.112563
8.594768	548.521147	10.117581
8.608412	547.005256	10.122599
8.336889	536.219159	10.127616
8.497514	541.757153	10.132634
8.652144	542.041012	10.137651
8.526562	536.378798	10.142669
8.730507	526.310765	10.147687
8.574834	528.957648	10.152704
7.946349	524.634135	10.157722
8.433513	534.115789	10.162739
8.172576	546.803389	10.167757
8.431613	538.663092	10.172775
8.553888	549.411390	10.177792
8.728482	546.211881	10.182810
8.627432	550.224230	10.187827
8.806587	553.816584	10.192845
9.015686	546.137276	10.197863
8.605676	549.203417	10.202880
8.920448	548.708844	10.207898
8.753687	549.673438	10.212915
8.301941	527.071400	10.217933
8.946837	532.100293	10.222951
8.481149	538.588000	10.227968
8.875228	540.933432	10.232986
8.694442	539.248966	10.238003
8.117005	538.835804	10.243021
8.414900	541.287512	10.248039
8.525283	553.802220	10.253056
8.798622	541.836995	10.258074
8.712109	544.535417	10.263091
8.807778	544.290496	10.268109
8.923124	538.452174	10.273127
8.743133	550.539408	10.278144
9.114876	545.303068	10.283162
8.901237	549.101597	10.288179
8.846834	550.308983	10.293197
8.685474	543.728742	10.298215
8.386911	547.462598	10.303232
8.953208	542.524726	10.308250
8.652822	548.702014	10.313267
8.526623	546.524686	10.318285
8.961960	538.299687	10.323303
8.779252	541.439006	10.328320
8.800704	551.035778	10.333338
8.887954	546.341000	10.338355
8.636704	545.624826	10.343373
8.719314	539.993878	10.348391
8.874271	546.472507	10.353408
8.924546	546.494927	10.358426
9.185413	541.637749	10.363443
8.739700	549.725776	10.368461
9.254461	543.527239	10.373479
8.813544	551.677460	10.378496
8.692361	548.272027	10.383514
8.701195	539.386211	10.388531
9.023339	543.337731	10.393549
8.934604	538.885467	10.398567
8.552527	546.153762	10.403584
8.574480	543.201955	10.408602
8.800016	537.066667	10.413619
8.460188	550.425553	10.418637
8.769256	544.870285	10.423655
8.721516	544.586715	10.428672
8.662226	547.782561	10.433690
9.029572	562.274066	10.438707
9.065951	574.429025	10.443725
9.218404	570.043695	10.448743
8.814543	565.066089	10.453760
8.662359	572.625241	10.458778
9.343375	576.782087	10.463795
8.977324	584.303436	10.468813
9.260689	573.401609	10.473831
9.319766	570.602890	10.478848
8.758878	554.992013	10.483866
9.138683	560.483483	10.488883
9.074482	574.306947	10.493901
9.271756	569.566582	10.498919
9.194929	560.457752	10.503936
8.785092	557.523510	10.508954
8.965391	560.978482	10.513971
8.919502	572.229412	10.518989
9.159483	579.898024	10.524007
9.020569	586.150943	10.529024
9.066900	582.270550	10.534042
9.052213	586.079053	10.539059
8.775876	589.277781	10.544077
8.977407	579.042802	10.549095
8.835562	582.726308	10.554112
8.652620	586.538462	10.559130
9.121748	583.519881	10.564147
8.819191	583.744025	10.569165
9.510044	594.986152	10.574183
9.227175	588.960424	10.579200
9.390158	595.707018	10.584218
9.381382	574.626919	10.589235
9.224720	583.233003	10.594253
9.021364	574.319710	10.599271
9.289053	576.970900	10.604288
8.963197	578.080730	10.609306
9.091357	587.561240	10.614323
9.532486	607.208909	10.619341
9.449927	602.003688	10.624359
9.779423	588.443411	10.629376
9.490862	590.086004	10.634394
9.510392	577.103012	10.639411
9.042610	575.607593	10.644429
9.472353	579.046260	10.649447
9.859657	582.420504	10.654464
9.644929	577.669627	10.659482
9.797983	573.650116	10.664499
9.219012	580.654005	10.669517
9.509182	571.551123	10.674535
9.822528	577.999207	10.679552
9.436426	575.429510	10.684570
9.370268	587.118618	10.689587
9.466559	585.614431	10.694605
9.555681	575.214814	10.699623
9.949333	577.255226	10.704640
9.071339	569.530741	10.709658
9.187743	556.034123	10.714675
9.050178	572.351249	10.719693
9.402454	581.952900	10.724711
9.467624	577.252714	10.729728
9.096509	582.568561	10.734746
9.608390	567.671500	10.739763
9.401330	583.169101	10.744781
9.208328	577.049565	10.749799
9.331728	580.994441	10.754816
9.434757	578.840956	10.759834
9.510887	576.655313	10.764851
9.212465	577.941886	10.769869
9.118177	574.575888	10.774887
9.231886	587.787465	10.779904
9.237222	596.627933	10.784922
9.494782	599.332375	10.789939
9.383652	599.814564	10.794957
9.559281	605.565042	10.799975
9.478258	604.724816	10.804992
9.432617	609.863556	10.810010
9.761579	607.948028	10.815027
9.755890	607.682689	10.820045
9.656672	609.235863	10.825063
9.904788	608.403925	10.830080
9.598317	612.326889	10.835098
9.341436	600.065589	10.840115
9.304509	604.748585	10.845133
9.520425	607.772501	10.850151
9.542348	605.185820	10.855168
9.050470	614.387354	10.860186
9.269589	617.974877	10.865203
9.347344	640.732357	10.870221
9.499582	635.080200	10.875239
9.487207	641.758614	10.880256
9.547313	651.104970	10.885274
9.751602	638.924151	10.890291
9.865875	646.820095	10.895309
9.976209	636.147652	10.900327
9.836149	645.729499	10.905344
9.767789	644.821628	10.910362
9.949172	637.074822	10.915379
9.731083	648.250785	10.920397
10.127714	643.866533	10.925415
10.254724	647.124457	10.930432
9.944495	647.816967	10.935450
10.337379	638.594878	10.940467
9.926274	633.754660	10.945485
10.064072	632.137893	10.950503
10.217897	608.785894	10.955520
9.482624	611.383307	10.960538
9.824332	600.033445	10.965555
9.800375	621.392680	10.970573
9.983909	613.254415	10.975591
9.881286	620.922698	10.980608
9.944560	637.578459	10.985626
10.320227	636.278184	10.990643
10.050934	616.054106	10.995661
9.819171	608.435174	11.000679
9.734608	602.123077	11.005696
9.560349	614.129495	11.010714
9.907286	621.624916	11.015731
9.948865	641.197069	11.020749
10.164546	631.513613	11.025767
10.224096	629.274806	11.030784
9.791929	639.138863	11.035802
10.013939	631.337304	11.040819
10.148697	629.866307	11.045837
10.238408	629.409197	11.050855
10.116395	629.171978	11.055872
10.162187	636.307065	11.060890
10.438358	628.340053	11.065907
10.090200	622.448934	11.070925
9.963747	603.766074	11.075943
10.011946	615.538032	11.080960
9.917900	625.825387	11.085978
10.198345	626.360050	11.090995
10.139061	638.786592	11.096013
9.819517	637.341811	11.101031
10.097132	631.967298	11.106048
10.100366	637.620754	11.111066
10.385613	624.824218	11.116083
10.116676	637.838785	11.121101
10.169255	631.184893	11.126119
10.161531	630.178405	11.131136
10.204875	633.692683	11.136154
10.300260	631.012933	11.141171
10.188913	628.635902	11.146189
9.939888	625.821859	11.151207
10.366242	628.663501	11.156224
10.189572	627.750143	11.161242
9.956408	623.528450	11.166259
10.387266	632.293554	11.171277
10.089769	631.220491	11.176295
10.251743	626.114523	11.181312
10.273460	632.442822	11.186330
10.278863	632.260483	11.191347
10.439560	627.814524	11.196365
10.252971	633.008696	11.201383
10.022612	627.721845	11.206400
10.105875	629.068438	11.211418
9.973064	630.533876	11.216435
9.965988	625.360436	11.221453
10.178671	640.295314	11.226471
10.383386	645.633144	11.231488
10.160698	652.624323	11.236506
10.303461	655.911921	11.241523
10.275862	654.110744	11.246541
10.333385	659.403665	11.251559
10.506545	658.699484	11.256576
10.379780	671.078962	11.261594
10.378375	652.851486	11.266611
10.691369	658.881186	11.271629
10.486211	662.253759	11.276647
10.758446	657.383639	11.281664
10.567785	667.153789	11.286682
10.375945	660.227190	11.291699
10.551774	660.258148	11.296717
10.710065	656.908374	11.301735
10.766416	657.924605	11.306752
10.481220	663.068191	11.311770
10.388605	660.352051	11.316787
10.601681	660.989794	11.321805
10.609536	658.049157	11.326823
10.994361	660.720529	11.331840
10.943523	664.493702	11.336858
10.638862	648.780657	11.341875
10.643261	634.824203	11.346893
10.279136	629.543756	11.351911
10.576165	637.455492	11.356928
10.586064	653.405197	11.361946
10.925683	654.146582	11.366963
11.016978	656.707318	11.371981
10.546099	645.877389	11.376999
10.408602	636.278397	11.382016
9.996956	645.004096	11.387034
10.601077	661.794717	11.392051
10.738275	662.042098	11.397069
10.640051	663.363435	11.402087
10.767930	655.744567	11.407104
10.673429	665.127162	11.412122
10.678856	668.094614	11.417139
10.681134	657.351472	11.422157
10.584162	660.917927	11.427175
10.414453	663.478580	11.432192
10.582450	663.586618	11.437210
10.341958	664.731527	11.442227
10.326355	666.741106	11.447245
10.843536	687.794696	11.452263
10.823045	693.067873	11.457280
10.736378	692.811021	11.462298
10.688871	704.919347	11.467315
11.019458	703.731643	11.472333
11.132473	703.975155	11.477351
10.986147	695.325560	11.482368
10.815177	699.478454	11.487386
10.773375	699.118509	11.492403
10.823467	693.046462	11.497421
10.724700	704.431433	11.502439
10.957832	700.813170	11.507456
11.092454	691.580867	11.512474
11.030262	702.995604	11.517491
11.075795	690.129858	11.522509
10.891360	700.342473	11.527527
11.000472	692.160785	11.532544
11.130164	698.684605	11.537562
11.219073	692.751790	11.542579
10.947039	686.874023	11.547597
10.766254	693.151241	11.552615
10.951208	687.006473	11.557632
11.054480	694.046050	11.562650
11.145721	690.952041	11.567667
11.036394	693.481442	11.572685
10.867248	698.056448	11.577703
10.960464	696.750975	11.582720
11.124965	690.047818	11.587738
11.004179	692.412591	11.592755
11.398064	691.874601	11.597773
11.051852	691.954410	11.602791
11.602432	693.954876	11.607808
11.215729	687.828398	11.612826
11.220881	691.212015	11.617843
11.326959	692.407009	11.622861
10.999960	681.541813	11.627879
11.346073	678.817386	11.632896
11.307739	679.896145	11.637914
10.959072	682.740357	11.642931
11.181993	681.846450	11.647949
11.239166	690.219952	11.652967
11.468414	688.343957	11.657984
11.230945	699.246018	11.663002
11.038040	696.482114	11.668019
11.239883	695.657047	11.673037
11.074932	689.415112	11.678055
11.320235	692.211752	11.683072
11.209759	690.744352	11.688090
11.045464	693.387574	11.693107
11.271663	691.350676	11.698125
11.222473	701.230285	11.703143
11.594681	683.824511	11.708160
11.523001	689.858477	11.713178
11.245689	693.891193	11.718195
11.304279	681.953548	11.723213
10.972809	684.871679	11.728231
11.302598	686.487866	11.733248
11.365316	691.877177	11.738266
11.122071	697.190785	11.743283
11.386858	695.321895	11.748301
11.372479	705.037091	11.753319
11.320027	691.815545	11.758336
11.233099	700.877440	11.763354
11.054005	702.360194	11.768371
11.314293	699.979483	11.773389
11.366159	710.976152	11.778407
11.754766	703.778032	11.783424
11.771551	719.810518	11.788442
11.604656	708.546372	11.793459
11.620110	694.091609	11.798477
11.519113	697.701059	11.803495
11.445661	695.902745	11.808512
11.919545	695.886906	11.813530
11.613184	695.813275	11.818547
11.505546	687.178537	11.823565
11.649892	698.904324	11.828583
11.220429	690.008722	11.833600
11.409180	690.856189	11.838618
11.413584	711.945515	11.843635
11.669995	705.242485	11.848653
11.146624	717.538670	11.853671
11.628613	703.009398	11.858688
11.425763	713.400651	11.863706
11.468770	715.514303	11.868723
11.717570	709.507764	11.873741
11.455077	720.083296	11.878759
11.491993	721.866088	11.883776
11.867435	719.956826	11.888794
11.631216	720.360526	11.893811
11.449411	706.830880	11.898829
11.818577	714.430335	11.903847
11.738874	720.192824	11.908864
11.698022	715.207022	11.913882
11.425314	719.910200	11.918899
11.874826	725.273265	11.923917
11.704358	740.773429	11.928935
12.288111	734.577958	11.933952
12.252964	719.355612	11.938970
11.853492	717.277839	11.943987
12.102930	707.755664	11.949005
12.165447	709.946001	11.954023
11.809487	704.398247	11.959040
12.161344	707.633516	11.964058
12.151807	714.154809	11.969075
11.849191	704.899238	11.974093
11.951142	713.622402	11.979111
11.729604	712.176935	11.984128
11.936270	711.375869	11.989146
11.829507	713.841861	11.994163
11.863016	708.678797	11.999181
11.730947	706.786258	12.004199
11.830921	710.538405	12.009216
11.908145	706.377883	12.014234
11.740836	712.309984	12.019251
11.462437	728.186647	12.024269
11.561287	737.464242	12.029287
12.078874	734.009484	12.034304
12.426747	729.578561	12.039322
11.810594	738.412779	12.044339
12.069413	743.358242	12.049357
12.317009	739.495069	12.054375
12.363575	746.414147	12.059392
12.307236	747.367553	12.064410
12.270148	742.415763	12.069427
12.228995	742.029333	12.074445
12.497301	736.742345	12.079463
12.193210	730.360058	12.084480
12.384082	713.975163	12.089498
12.046766	721.605395	12.094515
12.176902	713.754446	12.099533
11.912469	719.940807	12.104551
12.528208	728.379306	12.109568
12.223733	717.797345	12.114586
12.022741	717.724768	12.119603
12.359962	733.256989	12.124621
12.499783	742.599057	12.129639
12.298166	725.308335	12.134656
12.144382	719.033045	12.139674
12.110608	723.400220	12.144691
12.184170	728.293290	12.149709
12.062353	746.877735	12.154727
12.310070	752.710025	12.159744
12.423433	747.011316	12.164762
12.254142	742.880188	12.169779
12.380071	741.723222	12.174797
12.218172	749.018139	12.179815
12.203842	741.132441	12.184832
12.422124	744.083556	12.189850
12.256879	750.712926	12.194867
12.404916	742.825141	12.199885
12.560436	745.908690	12.204903
12.202880	751.063697	12.209920
12.333480	745.378274	12.214938
12.510128	737.798728	12.219955
12.487134	748.456659	12.224973
12.071381	747.782675	12.229991
12.372218	742.919406	12.235008
12.468144	741.014697	12.240026
12.400686	754.034973	12.245043
12.656562	739.858052	12.250061
12.065289	747.960246	12.255079
12.098419	758.665580	12.260096
12.560264	771.157302	12.265114
12.628934	777.407418	12.270131
12.599284	773.614161	12.275149
12.326361	770.035983	12.280167
12.645366	777.161127	12.285184
12.855450	772.456963	12.290202
12.695640	771.488641	12.295219
13.059605	765.621662	12.300237
12.743032	771.776917	12.305255
12.638444	776.364089	12.310272
13.138411	774.116895	12.315290
12.686117	775.588994	12.320307
12.574835	777.891186	12.325325
12.767380	776.499577	12.330343
12.579432	771.957382	12.335360
12.588226	768.867956	12.340378
12.477102	772.206675	12.345395
12.703626	774.460015	12.350413
12.685947	765.593420	12.355431
12.677819	774.122654	12.360448
12.946836	767.123039	12.365466
12.795590	776.440496	12.370483
13.082250	778.082339	12.375501
12.917651	777.676982	12.380519
12.740471	772.433831	12.385536
13.073389	768.356928	12.390554
12.729354	774.056129	12.395571
12.554839	775.610962	12.400589
12.724185	771.767038	12.405607
12.843124	771.321422	12.410624
13.158381	760.863960	12.415642
12.701912	770.254790	12.420659
12.901709	771.895268	12.425677
13.039759	764.164236	12.430695
13.082295	768.586499	12.435712
13.217114	772.441940	12.440730
12.827979	774.136244	12.445747
13.043428	777.876372	12.450765
12.877898	763.585757	12.455783
13.042902	771.737522	12.460800
13.103725	767.252947	12.465818
12.762287	774.433914	12.470835
12.837488	773.658159	12.475853
12.830345	775.913187	12.480871
13.247194	796.673715	12.485888
13.401861	789.896557	12.490906
12.681952	786.720327	12.495923
13.111828	789.016369	12.500941
12.990865	798.657940	12.505959
13.217169	806.344874	12.510976
13.412318	802.282902	12.515994
13.348436	799.368881	12.521011
13.379253	800.513752	12.526029
13.424018	775.108223	12.531047
12.744275	783.730568	12.536064
13.127204	792.150964	12.541082
13.134298	797.692427	12.546099
13.555841	802.099969	12.551117
13.471487	799.929847	12.556135
13.180273	815.141829	12.561152
13.600048	796.416707	12.566170
13.235281	786.682824	12.571187
13.278212	784.132592	12.576205
13.197226	797.572443	12.581223
13.248271	796.430629	12.586240
13.565651	798.053214	12.591258
13.103038	807.510828	12.596275
13.510398	807.594977	12.601293
13.609644	808.309643	12.606311
13.411062	811.911659	12.611328
13.767143	799.510117	12.616346
13.858392	793.219416	12.621363
13.186337	782.224290	12.626381
13.360989	776.714228	12.631399
13.123355	788.499006	12.636416
13.134961	793.896028	12.641434
12.975200	802.731868	12.646451
13.181446	808.304526	12.651469
13.572402	801.059520	12.656487
13.451782	808.268106	12.661504
13.094172	800.755739	12.666522
13.197968	804.772616	12.671539
12.976551	811.743972	12.676557
13.803905	822.690254	12.681575
13.650251	836.930711	12.686592
13.731921	831.132500	12.691610
13.750857	837.533387	12.696627
13.606869	845.093873	12.701645
13.516283	842.169306	12.706663
13.812109	841.077501	12.711680
13.563579	833.361633	12.716698
13.434250	833.690551	12.721715
13.611686	833.203752	12.726733
13.885919	839.017119	12.731751
13.863164	834.016865	12.736768
13.775702	834.961652	12.741786
13.447273	840.277210	12.746803
13.587979	829.796641	12.751821
13.773634	828.966374	12.756839
13.391338	841.329447	12.761856
14.192685	829.861181	12.766874
14.069988	834.799774	12.771891
13.984366	836.143054	12.776909
13.654397	830.087828	12.781927
13.843264	837.775465	12.786944
13.886556	832.447757	12.791962
13.970333	833.018537	12.796979
13.532289	835.520903	12.801997
13.715001	829.272126	12.807015
13.703127	836.465473	12.812032
13.636095	832.268966	12.817050
13.780924	825.739471	12.822067
13.814352	838.224635	12.827085
13.890059	846.243203	12.832103
13.936859	863.961328	12.837120
14.285980	860.194301	12.842138
14.133824	859.735703	12.847155
13.914532	855.518735	12.852173
14.360758	853.123745	12.857191
13.960347	850.548890	12.862208
13.897642	843.620706	12.867226
14.013365	859.839698	12.872243
14.068543	866.776694	12.877261
14.416687	862.898022	12.882279
14.542659	860.402921	12.887296
14.415048	841.874682	12.892314
14.395029	834.321750	12.897331
14.224426	830.903376	12.902349
14.434259	825.945314	12.907367
14.031893	830.156244	12.912384
14.249935	834.749060	12.917402
13.822599	828.355646	12.922419
13.948773	833.839217	12.927437
14.226747	829.523379	12.932455
14.232438	839.103059	12.937472
14.435740	850.413708	12.942490
14.347279	828.016609	12.947507
14.131498	831.225829	12.952525
14.363878	838.950748	12.957543
14.653537	859.634003	12.962560
14.350625	845.722342	12.967578
14.363058	836.801116	12.972595
14.119128	843.145540	12.977613
14.483441	835.800210	12.982631
14.407069	855.315398	12.987648
14.636513	845.818889	12.992666
14.262577	834.039753	12.997683
14.353634	844.612727	13.002701
14.240646	853.322746	13.007719
14.364237	870.687236	13.012736
14.768658	856.110041	13.017754
14.792765	854.995123	13.022771
14.432766	857.790064	13.027789
14.530901	860.186717	13.032807
14.298699	862.784128	13.037824
14.386380	864.130600	13.042842
14.449085	860.618864	13.047859
14.416352	862.451787	13.052877
14.561367	862.015629	13.057895
14.413583	872.458102	13.062912
14.839571	859.939430	13.067930
14.754824	859.320071	13.072947
14.568412	855.952338	13.077965
14.545599	866.017833	13.082983
14.799660	877.221676	13.088000
14.700826	859.068552	13.093018
14.561411	867.984914	13.098035
14.352183	859.672397	13.103053
14.577993	865.561112	13.108071
14.489686	871.929775	13.113088
14.463666	862.635000	13.118106
14.384152	868.745525	13.123123
14.235959	887.775035	13.128141
14.848018	883.320793	13.133159
14.863895	891.488261	13.138176
14.773435	893.468928	13.143194
15.223598	892.760991	13.148211
14.657623	904.901787	13.153229
14.987279	899.081776	13.158247
15.142141	901.252519	13.163264
15.020340	895.908822	13.168282
15.079603	896.019513	13.173299
14.673556	891.146488	13.178317
14.995192	889.510669	13.183335
15.061141	897.018307	13.188352
15.090846	895.706800	13.193370
14.820524	896.786195	13.198387
14.976807	906.364208	13.203405
15.138093	894.658594	13.208423
14.975601	907.948265	13.213440
15.296115	901.640422	13.218458
14.850978	894.808612	13.223475
14.987893	901.864365	13.228493
15.099226	895.419911	13.233511
15.294137	897.776531	13.238528
14.823130	898.911599	13.243546
15.065282	893.106867	13.248563
14.759273	898.545892	13.253581
14.880000	896.030788	13.258599
15.010799	896.101683	13.263616
15.139644	897.538974	13.268634
15.302695	897.819478	13.273651
14.751763	899.914191	13.278669
15.063308	888.393138	13.283687
15.178307	895.832813	13.288704
15.031013	896.291867	13.293722
15.116999	889.054409	13.298739
15.077756	917.003652	13.303757
15.337322	922.098648	13.308775
15.479564	922.996742	13.313792
15.825768	923.972866	13.318810
15.742062	902.973229	13.323827
15.275725	901.493087	13.328845
15.387394	891.670795	13.333863
15.174362	886.889425	13.338880
15.071694	892.708927	13.343898
15.601610	900.225953	13.348915
15.432171	917.985066	13.353933
15.382422	900.029268	13.358951
15.620878	906.199355	13.363968
15.478549	909.970021	13.368986
15.609832	894.330200	13.374003
15.400102	893.468557	13.379021
15.253135	889.607302	13.384039
15.603938	905.922841	13.389056
15.623674	922.582969	13.394074
16.033143	912.153503	13.399091
15.362976	904.018861	13.404109
15.613521	898.564295	13.409127
15.727746	906.221022	13.414144
15.537936	908.318531	13.419162
16.030951	893.674271	13.424179
15.550525	893.143659	13.429197
15.445413	889.919535	13.434215
15.864089	903.141310	13.439232
15.498087	891.765127	13.444250
15.407068	905.428769	13.449267
15.602190	919.575722	13.454285
15.480132	915.576484	13.459303
15.428213	925.764547	13.464320
15.524380	926.684443	13.469338
15.535433	926.546438	13.474355
15.463983	922.986828	13.479373
15.666185	926.407547	13.484391
15.503129	928.759278	13.489408
15.520003	931.592608	13.494426
16.052831	942.666089	13.499443
15.570991	956.707076	13.504461
15.999385	959.029373	13.509479
15.798208	955.085744	13.514496
16.018781	957.759762	13.519514
16.377533	950.879845	13.524531
15.854000	951.927162	13.529549
16.218471	950.722412	13.534567
15.857245	949.634683	13.539584
15.813091	953.794596	13.544602
16.256408	953.583436	13.549619
16.170725	956.930187	13.554637
15.962233	951.004397	13.559655
16.028745	941.407651	13.564672
15.960433	948.071445	13.569690
16.318400	945.885929	13.574707
15.843589	953.098906	13.579725
16.400493	945.223231	13.584743
16.012278	953.160810	13.589760
15.666839	955.561643	13.594778
16.342695	949.098092	13.599795
16.292036	953.233887	13.604813
16.338650	946.697377	13.609831
16.244520	950.095522	13.614848
15.901770	959.255046	13.619866
16.226166	943.881214	13.624883
15.790577	950.303873	13.629901
15.849193	957.769450	13.634919
15.916273	950.179205	13.639936
16.035528	950.851983	13.644954
16.406372	944.770423	13.649971
16.129300	956.711851	13.654989
16.543769	967.388827	13.660007
16.615913	958.180885	13.665024
16.261839	959.959161	13.670042
16.727329	948.143293	13.675059
16.447485	954.405918	13.680077
16.412332	948.431348	13.685095
16.470056	946.414048	13.690112
16.292252	947.847008	13.695130
16.438911	945.876395	13.700147
16.366049	951.149671	13.705165
16.281954	969.297841	13.710183
16.629713	973.338533	13.715200
16.719183	978.351089	13.720218
16.806866	975.555631	13.725235
16.432170	972.567854	13.730253
16.847817	965.527729	13.735271
16.541446	948.564326	13.740288
16.231056	955.220180	13.745306
16.861101	960.809720	13.750323
16.894072	966.977639	13.755341
16.524122	962.535995	13.760359
16.715598	954.485011	13.765376
16.597020	972.299934	13.770394
16.986066	967.640483	13.775411
16.601026	958.338569	13.780429
16.860413	978.047513	13.785447
17.020746	958.866361	13.790464
16.416295	956.000094	13.795482
16.772783	960.837726	13.800499
16.655732	973.151863	13.805517
16.694356	976.491024	13.810535
16.481897	964.466555	13.815552
16.691275	970.718251	13.820570
17.359857	960.942271	13.825587
17.233010	972.164379	13.830605
16.986924	976.989992	13.835623
16.963316	977.742725	13.840640
16.974046	982.236062	13.845658
17.168072	968.729775	13.850675
16.998642	968.626380	13.855693
16.866812	961.268665	13.860711
17.105225	963.999964	13.865728
16.711123	979.899979	13.870746
16.888430	977.383368	13.875763
17.247248	978.691644	13.880781
16.847338	975.028545	13.885799
16.818477	966.531780	13.890816
17.015649	977.895110	13.895834
17.123835	975.901733	13.900851
17.175069	978.936458	13.905869
17.083540	972.975938	13.910887
16.927506	973.289991	13.915904
17.123858	978.565544	13.920922
16.898719	976.510045	13.925939
17.376419	979.658395	13.930957
17.317973	972.329072	13.935975
17.399376	973.312043	13.940992
16.882616	967.279033	13.946010
17.600676	969.216767	13.951027
17.043001	970.044552	13.956045
17.086718	971.086123	13.961063
17.438928	967.747673	13.966080
17.270786	970.154580	13.971098
17.117349	968.446248	13.976115
17.171444	977.662109	13.981133
17.299290	988.264520	13.986151
17.431509	997.659968	13.991168
17.495436	1004.088906	13.996186
17.645820	999.663445	14.001203
17.650919	994.843165	14.006221
17.563610	990.455887	14.011239
17.535648	971.992089	14.016256
17.670825	974.355856	14.021274
17.450079	963.413027	14.026291
17.131647	973.644860	14.031309
17.360133	974.848740	14.036327
17.493127	993.903074	14.041344
17.483873	992.984607	14.046362
17.764108	991.943796	14.051379
17.846984	997.388534	14.056397
17.669299	999.275396	14.061415
17.926701	992.677979	14.066432
17.898812	995.455743	14.071450
17.836920	999.720570	14.076467
17.789868	998.072567	14.081485
18.025015	1006.392754	14.086503
17.949819	981.102417	14.091520
17.236458	978.173081	14.096538
17.807366	980.633193	14.101555
17.885604	989.599011	14.106573
17.700131	999.143913	14.111591
17.603124	991.604047	14.116608
17.621979	1006.732589	14.121626
17.776864	1004.092526	14.126643
17.354867	997.244634	14.131661
17.569050	1003.547120	14.136679
17.727194	989.596383	14.141696
17.750862	997.431529	14.146714
17.552393	1000.217069	14.151731
17.529712	1010.081462	14.156749
17.582199	1026.834306	14.161767
17.946966	1023.274089	14.166784
17.779936	1034.829654	14.171802
17.812114	1036.145964	14.176819
18.057447	1029.988307	14.181837
18.038360	1035.363332	14.186855
18.084440	1019.120197	14.191872
18.127703	1025.947431	14.196890
18.069415	1025.707919	14.201907
18.258469	1024.197974	14.206925
17.838189	1038.009558	14.211943
18.223724	1024.972671	14.216960
18.338232	1036.665468	14.221978
18.040214	1029.669084	14.226995
18.287962	1038.336400	14.232013
18.319093	1033.270862	14.237031
18.403597	1023.819899	14.242048
18.193234	1028.373087	14.247066
18.464264	1027.260574	14.252083
18.795380	1027.206177	14.257101
18.332391	1036.892721	14.262119
18.450536	1018.216887	14.267136
18.338465	1026.809140	14.272154
18.273864	1021.474431	14.277171
18.421867	1019.383907	14.282189
18.348662	1028.998028	14.287207
18.528539	1023.865738	14.292224
18.413591	1025.662296	14.297242
18.268323	1024.002996	14.302259
18.736210	1025.134955	14.307277
18.571682	1028.438873	14.312295
18.466908	1029.479054	14.317312
18.369450	1017.840601	14.322330
18.352422	1027.744619	14.327347
18.354567	1030.905983	14.332365
18.433759	1040.338189	14.337383
18.542595	1049.152918	14.342400
18.527910	1052.638714	14.347418
18.942064	1052.009958	14.352435
19.116618	1043.789691	14.357453
18.757320	1047.419948	14.362471
18.769515	1034.079929	14.367488
18.590121	1036.961919	14.372506
18.966538	1046.027995	14.377523
18.770665	1037.867495	14.382541
18.577321	1040.853760	14.387559
18.925294	1034.698790	14.392576
18.618065	1045.798465	14.397594
18.577379	1052.349859	14.402611
18.950927	1047.599254	14.407629
18.572002	1058.023436	14.412647
19.140033	1051.785171	14.417664
18.866969	1051.273362	14.422682
18.703326	1057.059718	14.427699
19.202808	1055.255856	14.432717
19.178480	1063.154099	14.437735
19.141831	1050.205210	14.442752
18.786482	1053.906859	14.447770
18.627928	1055.168537	14.452787
18.813715	1050.961206	14.457805
18.717184	1047.479339	14.462823
18.872948	1046.695348	14.467840
19.020844	1056.239410	14.472858
19.162323	1054.792456	14.477875
19.051055	1054.198740	14.482893
18.948077	1055.385863	14.487911
19.029196	1054.569352	14.492928
18.829394	1063.515903	14.497946
18.893463	1074.511990	14.502963
19.526917	1069.851405	14.507981
19.298239	1082.714408	14.512999
19.268209	1078.856575	14.518016
19.577241	1074.342621	14.523034
19.220728	1074.070606	14.528051
19.507603	1073.490090	14.533069
19.097193	1075.529667	14.538087
19.438469	1077.292809	14.543104
19.459773	1077.238534	14.548122
19.120210	1081.558812	14.553139
19.386404	1076.621652	14.558157
19.482816	1080.041421	14.563175
19.283116	1077.997443	14.568192
19.697855	1075.528503	14.573210
19.396043	1077.464273	14.578227
19.402393	1072.342199	14.583245
19.411065	1081.547534	14.588263
19.709645	1075.662134	14.593280
19.805807	1076.592276	14.598298
19.507948	1074.449596	14.603315
19.667834	1064.553465	14.608333
19.697945	1074.737491	14.613351
19.832060	1072.656740	14.618368
19.894543	1074.583759	14.623386
19.830640	1064.686892	14.628403
19.925107	1073.602436	14.633421
19.732518	1060.146311	14.638439
19.931498	1048.060338	14.643456
20.254444	1036.169980	14.648474
19.524300	1042.082814	14.653491
19.784951	1043.950244	14.658509
19.375969	1035.858891	14.663527
19.746968	1037.202950	14.668544
19.699834	1060.216560	14.673562
19.688170	1067.409586	14.678579
19.907310	1066.525733	14.683597
19.936475	1077.187458	14.688615
19.939874	1067.931387	14.693632
19.968791	1072.913845	14.698650
19.622424	1073.201545	14.703667
19.926445	1066.402291	14.708685
19.984501	1075.355754	14.713703
19.954113	1075.226184	14.718720
19.843502	1068.856992	14.723738
20.064751	1067.646030	14.728755
20.519043	1065.802408	14.733773
20.170977	1072.805088	14.738791
20.196210	1077.314161	14.743808
20.163052	1063.855647	14.748826
20.265586	1071.065196	14.753843
20.220924	1063.564657	14.758861
19.935891	1074.492967	14.763879
19.832095	1070.862697	14.768896
20.358648	1065.970612	14.773914
20.402116	1072.488790	14.778931
20.333275	1058.281888	14.783949
19.920507	1070.901753	14.788967
20.001283	1063.913492	14.793984
20.367781	1070.804539	14.799002
20.062878	1069.772826	14.804019
20.303901	1065.371313	14.809037
20.148763	1071.014932	14.814055
20.208251	1086.084463	14.819072
20.260745	1091.673237	14.824090
20.511697	1098.997587	14.829107
20.712525	1095.267264	14.834125
20.736104	1097.820390	14.839143
20.453084	1089.763660	14.844160
20.459725	1083.881720	14.849178
20.470083	1099.775510	14.854195
20.944792	1093.766454	14.859213
20.673929	1085.455360	14.864231
20.500790	1074.077026	14.869248
20.388531	1074.664923	14.874266
20.592997	1089.003784	14.879283
20.856214	1087.624854	14.884301
20.664417	1100.373107	14.889319
20.672657	1108.639982	14.894336
20.836359	1098.062120	14.899354
20.514775	1095.853684	14.904371
21.083214	1097.611100	14.909389
20.440949	1101.345705	14.914407
20.945827	1100.297215	14.919424
20.641936	1097.731925	14.924442
20.350714	1105.607458	14.929459
20.685994	1097.337714	14.934477
20.646446	1102.801580	14.939495
20.605998	1094.650745	14.944512
20.683388	1093.750994	14.949530
20.567271	1097.953963	14.954547
21.009054	1093.712892	14.959565
20.614021	1095.073966	14.964583
20.869521	1118.453281	14.969600
21.076342	1114.885735	14.974618
20.835954	1131.145476	14.979635
21.315114	1126.362793	14.984653
20.981872	1132.573309	14.989671
21.198370	1123.585057	14.994688
21.597621	1127.063347	14.999706
21.390561	1123.737555	15.004723
21.281548	1103.473701	15.009741
21.142625	1103.031407	15.014759
21.156771	1097.888742	15.019776
21.032228	1101.154166	15.024794
21.315836	1123.375728	15.029811
21.433503	1118.175364	15.034829
21.156041	1123.683752	15.039847
21.767462	1125.331696	15.044864
21.375774	1110.787669	15.049882
21.181586	1105.169676	15.054899
21.177333	1103.364974	15.059917
21.338449	1118.377158	15.064935
21.362908	1119.916005	15.069952
21.659463	1125.070296	15.074970
21.506911	1134.761399	15.079987
21.490925	1125.558896	15.085005
21.570127	1125.736757	15.090023
21.426547	1131.077314	15.095040
21.409707	1122.849329	15.100058
21.625740	1129.862559	15.105075
21.739856	1123.669510	15.110093
21.491113	1123.586727	15.115111
21.524197	1133.410076	15.120128
21.428129	1125.718025	15.125146
21.362619	1132.914487	15.130163
21.749305	1123.881124	15.135181
21.353415	1129.089057	15.140199
21.397281	1127.992107	15.145216
21.550433	1119.060408	15.150234
21.986798	1126.218247	15.155251
21.858151	1121.679514	15.160269
21.472927	1130.483585	15.165287
21.262966	1124.543012	15.170304
22.048101	1139.608179	15.175322
22.011821	1142.350745	15.180339
22.200959	1134.982710	15.185357
21.751123	1133.012033	15.190375
21.954229	1126.469613	15.195392
21.961171	1122.044643	15.200410
21.742564	1123.147772	15.205427
21.728824	1137.948781	15.210445
22.081400	1145.543718	15.215463
21.861303	1149.860372	15.220480
22.337012	1147.760053	15.225498
21.898507	1149.016523	15.230515
22.146719	1149.980150	15.235533
22.243516	1146.444595	15.240551
22.125370	1147.028352	15.245568
22.296952	1153.832425	15.250586
22.355170	1149.474938	15.255603
21.948366	1144.127564	15.260621
21.986306	1152.328522	15.265639
21.893808	1144.964206	15.270656
22.349232	1145.555738	15.275674
22.262826	1149.993163	15.280691
22.477041	1146.379111	15.285709
22.302615	1138.859867	15.290727
22.249592	1152.310354	15.295744
22.087268	1141.116000	15.300762
22.009117	1136.869678	15.305779
22.126803	1133.552706	15.310797
22.245053	1136.392513	15.315815
22.421814	1154.790214	15.320832
22.652952	1161.865128	15.325850
22.732814	1153.396319	15.330867
22.660690	1147.666762	15.335885
22.432458	1141.363472	15.340903
22.355557	1138.091712	15.345920
22.708998	1154.257476	15.350938
22.975578	1161.490689	15.355955
22.603036	1145.976561	15.360973
22.596519	1140.272756	15.365991
22.070356	1139.220986	15.371008
22.610048	1152.993784	15.376026
22.960670	1161.958298	15.381043
22.753843	1164.014172	15.386061
23.059225	1160.896421	15.391079
22.795474	1172.396453	15.396096
22.882504	1164.858703	15.401114
22.903020	1164.405360	15.406131
22.937970	1171.082464	15.411149
23.084898	1168.714155	15.416167
22.596591	1174.677146	15.421184
23.208883	1163.858821	15.426202
23.030455	1163.677389	15.431219
22.924922	1159.171431	15.436237
23.306213	1154.174244	15.441255
22.934077	1166.727224	15.446272
23.323027	1157.456861	15.451290
23.310584	1158.818758	15.456307
23.396698	1147.251381	15.461325
23.189569	1130.961084	15.466343
23.042089	1131.691031	15.471360
23.049917	1126.241146	15.476378
22.939739	1137.697220	15.481395
22.870324	1150.488632	15.486413
22.871033	1157.100930	15.491431
22.955034	1167.537502	15.496448
23.324230	1158.239702	15.501466
23.372424	1167.158238	15.506483
23.163202	1164.556001	15.511501
22.984225	1166.799384	15.516519
23.102580	1165.019646	15.521536
23.262819	1160.648018	15.526554
23.281946	1166.762011	15.531571
23.261583	1161.003013	15.536589
23.259395	1166.267808	15.541607
23.198072	1173.492728	15.546624
23.585760	1189.716636	15.551642
23.163287	1195.677788	15.556659
23.341834	1197.986379	15.561677
23.447824	1195.820114	15.566695
23.321223	1189.772801	15.571712
23.465368	1190.664690	15.576730
23.426474	1196.094230	15.581747
23.565912	1193.601177	15.586765
23.605413	1193.065557	15.591783
23.625051	1196.810260	15.596800
23.856806	1194.348375	15.601818
23.374462	1200.833601	15.606835
23.476883	1196.108163	15.611853
23.440108	1203.743586	15.616871
23.333103	1218.676254	15.621888
23.670527	1225.651316	15.626906
23.846645	1223.354541	15.631923
24.119662	1226.255742	15.636941
24.178965	1212.287315	15.641959
24.142089	1223.581711	15.646976
24.266234	1214.942154	15.651994
24.466969	1215.821525	15.657011
24.278436	1191.431082	15.662029
24.150072	1180.085804	15.667047
24.064715	1183.890015	15.672064
24.168529	1177.690776	15.677082
23.905940	1179.780689	15.682099
23.921530	1179.141159	15.687117
24.085360	1181.759654	15.692135
23.978681	1180.264020	15.697152
23.933241	1189.873250	15.702170
24.428318	1203.372781	15.707187
24.618091	1210.663616	15.712205
24.449068	1197.503066	15.717223
24.300732	1183.594244	15.722240
24.213349	1183.774102	15.727258
24.022643	1177.655915	15.732275
24.198717	1201.876435	15.737293
24.621121	1202.473437	15.742311
24.253295	1211.039640	15.747328
24.459405	1202.819575	15.752346
24.481339	1210.096865	15.757363
24.727964	1211.876090	15.762381
24.503210	1209.540189	15.767399
24.484136	1211.388606	15.772416
24.885073	1206.588538	15.777434
24.608317	1213.569237	15.782451
24.807527	1215.165374	15.787469
24.657502	1178.957904	15.792487
24.336711	1178.721702	15.797504
24.765137	1197.283679	15.802522
24.694167	1208.926613	15.807539
24.782897	1209.648945	15.812557
24.641734	1204.948879	15.817575
24.541489	1219.517447	15.822592
24.659047	1208.111743	15.827610
24.771530	1211.724937	15.832627
24.719625	1209.776937	15.837645
24.883304	1203.383134	15.842663
24.805740	1218.642019	15.847680
24.668867	1210.309852	15.852698
24.591092	1210.273165	15.857715
24.656846	1212.028011	15.862733
24.884403	1208.916445	15.867751
24.817136	1214.629815	15.872768
25.090628	1205.659636	15.877786
25.080347	1207.889263	15.882803
24.708047	1208.255273	15.887821
25.021293	1201.513880	15.892839
24.982998	1210.814468	15.897856
25.065351	1223.430814	15.902874
25.168783	1232.153632	15.907891
25.133960	1233.962535	15.912909
25.244029	1225.936309	15.917927
25.358695	1246.001834	15.922944
25.362395	1240.115597	15.927962
25.364408	1228.178632	15.932979
25.537474	1241.344522	15.937997
25.720428	1226.780819	15.943015
25.350447	1209.608770	15.948032
25.325153	1205.903660	15.953050
25.251293	1198.977951	15.958067
25.398977	1221.600103	15.963085
25.600273	1223.543130	15.968103
25.163910	1238.113438	15.973120
25.342551	1230.402223	15.978138
25.660989	1228.862567	15.983155
25.649458	1238.723291	15.988173
25.674031	1225.112562	15.993191
25.622449	1240.202997	15.998208
25.671377	1222.515516	16.003226
25.648243	1228.285361	16.008243
25.398801	1230.210116	16.013261
25.905462	1225.525602	16.018279
26.267832	1231.360742	16.023296
25.624182	1231.429175	16.028314
25.705524	1233.466868	16.033331
25.642972	1236.496470	16.038349
25.849059	1225.126486	16.043367
25.652104	1233.889992	16.048384
26.051627	1223.268665	16.053402
25.878481	1224.639462	16.058419
25.866670	1235.880112	16.063437
25.874139	1215.358246	16.068455
25.614147	1225.300261	16.073472
25.645223	1219.364618	16.078490
25.819810	1218.434592	16.083507
25.684063	1234.845220	16.088525
25.703027	1241.843497	16.093543
25.667675	1257.202120	16.098560
26.079094	1251.820790	16.103578
26.181054	1258.312825	16.108595
26.153596	1262.348012	16.113613
26.256261	1257.574091	16.118631
26.024697	1260.772626	16.123648
26.140765	1257.681087	16.128666
26.347241	1254.008451	16.133683
26.584055	1253.128353	16.138701
26.789367	1247.076842	16.143719
26.479410	1248.904930	16.148736
26.455253	1249.531393	16.153754
26.490487	1242.712399	16.158771
26.075429	1253.044666	16.163789
26.779037	1244.431576	16.168807
26.614053	1256.381051	16.173824
26.548925	1249.928664	16.178842
26.865436	1250.993584	16.183859
26.551032	1249.042590	16.188877
26.512737	1248.144271	16.193895
26.534488	1246.776572	16.198912
26.471237	1254.052241	16.203930
26.734047	1244.699173	16.208947
26.730833	1250.880283	16.213965
26.579415	1246.100015	16.218983
26.705557	1244.635112	16.224000
26.803966	1250.135239	16.229018
26.931446	1251.742077	16.234035
26.865550	1252.509307	16.239053
26.891353	1240.858936	16.244071
26.865508	1246.274522	16.249088
26.671925	1243.552362	16.254106
27.090807	1255.231536	16.259123
26.719223	1251.000702	16.264141
27.179852	1246.911190	16.269159
27.085080	1247.767844	16.274176
26.997147	1245.592346	16.279194
26.717015	1249.396937	16.284211
26.899822	1246.212067	16.289229
27.197758	1246.739526	16.294247
27.120058	1244.674536	16.299264
26.966956	1236.071034	16.304282
27.161579	1251.633296	16.309299
27.485833	1276.343949	16.314317
27.282059	1245.081712	16.319335
27.235031	1254.867225	16.324352
27.172759	1245.361299	16.329370
27.152952	1251.507757	16.334387
27.164801	1271.197043	16.339405
27.328934	1278.461055	16.344423
27.786756	1273.528321	16.349440
27.523290	1273.112550	16.354458
27.565670	1263.434958	16.359475
27.343563	1275.886413	16.364493
27.423835	1269.985516	16.369511
27.558464	1276.696553	16.374528
27.392222	1271.429374	16.379546
27.772894	1276.946549	16.384563
27.344225	1281.444624	16.389581
27.448129	1272.563117	16.394599
27.587237	1279.499786	16.399616
27.386777	1270.625767	16.404634
27.551774	1271.479564	16.409651
27.529184	1274.194297	16.414669
27.550481	1278.613137	16.419687
27.691583	1283.165680	16.424704
27.464641	1298.799370	16.429722
27.934861	1292.292568	16.434739
27.915479	1308.629676	16.439757
27.957696	1298.561547	16.444775
28.094727	1306.733581	16.449792
27.790319	1303.018368	16.454810
28.013675	1300.543685	16.459827
27.713709	1296.789943	16.464845
28.019967	1298.415213	16.469863
27.923308	1295.119133	16.474880
27.711648	1300.982032	16.479898
28.369958	1296.318842	16.484915
28.189129	1303.271098	16.489933
28.036528	1301.236613	16.494951
28.017870	1295.761921	16.499968
28.092389	1296.985023	16.504986
28.130453	1296.397671	16.510003
28.358205	1311.800968	16.515021
28.342858	1325.531187	16.520039
28.549369	1319.896763	16.525056
28.633178	1314.056286	16.530074
28.462933	1297.960488	16.535091
28.621321	1290.665580	16.540109
28.290952	1283.259486	16.545127
28.382370	1293.615783	16.550144
28.396109	1303.114105	16.555162
28.801947	1306.516544	16.560179
28.755149	1303.841325	16.565197
28.516156	1287.377797	16.570215
28.650137	1292.523239	16.575232
28.596161	1288.613022	16.580250
28.655043	1295.362987	16.585267
28.478881	1315.003542	16.590285
28.703589	1310.480649	16.595303
28.438044	1317.037894	16.600320
28.645893	1314.794511	16.605338
28.925506	1313.130570	16.610355
28.641198	1326.126605	16.615373
28.863666	1323.404039	16.620391
29.045648	1323.066471	16.625408
28.908201	1314.961502	16.630426
28.818509	1309.712342	16.635443
29.018683	1316.549154	16.640461
29.264687	1315.774222	16.645479
29.061189	1313.729660	16.650496
28.616452	1316.754062	16.655514
29.371915	1314.363308	16.660531
29.342554	1315.224882	16.665549
29.009096	1315.365175	16.670567
29.333268	1309.610487	16.675584
29.036296	1316.933941	16.680602
29.073143	1311.815792	16.685619
28.812641	1321.247728	16.690637
29.282943	1334.700691	16.695655
29.447413	1340.817851	16.700672
29.553626	1345.332096	16.705690
29.672142	1347.457346	16.710707
29.368911	1326.337977	16.715725
29.276967	1320.677779	16.720743
29.176494	1326.983289	16.725760
29.302039	1349.691970	16.730778
29.249724	1340.395357	16.735795
29.451829	1345.263794	16.740813
29.296518	1349.245373	16.745831
29.712096	1336.302068	16.750848
29.430859	1339.861592	16.755866
29.778326	1338.330504	16.760883
29.750749	1343.501141	16.765901
29.690315	1337.901858	16.770919
29.839222	1337.005605	16.775936
29.597419	1344.237656	16.780954
29.670554	1344.052753	16.785971
29.745404	1350.511916	16.790989
29.831323	1353.266961	16.796007
30.524956	1358.836278	16.801024
30.074395	1357.930236	16.806042
29.898839	1341.912436	16.811059
29.931314	1343.418088	16.816077
29.640097	1340.746329	16.821095
30.248098	1355.589865	16.826112
30.110792	1367.986407	16.831130
30.407848	1361.888165	16.836147
30.210898	1369.998609	16.841165
30.309400	1358.787285	16.846183
30.683054	1356.782970	16.851200
30.235672	1352.014671	16.856218
29.926335	1336.321384	16.861235
30.145940	1346.863967	16.866253
30.296399	1363.375760	16.871271
30.618169	1368.275569	16.876288
30.523311	1365.753964	16.881306
30.072912	1361.734177	16.886323
30.143328	1359.294652	16.891341
30.220589	1367.201031	16.896359
30.492642	1362.973821	16.901376
30.032251	1369.312570	16.906394
30.363375	1370.875069	16.911411
30.553057	1362.059621	16.916429
30.137262	1365.206008	16.921447
30.162759	1367.086827	16.926464
30.415749	1386.324527	16.931482
30.641553	1391.298894	16.936499
30.852158	1392.852219	16.941517
30.503226	1401.135088	16.946535
30.636725	1398.090633	16.951552
30.720332	1395.743798	16.956570
30.759482	1393.829909	16.961587
30.620939	1387.063249	16.966605
30.779346	1392.172396	16.971623
30.883991	1391.731887	16.976640
30.945810	1396.264521	16.981658
30.995781	1387.515498	16.986675
31.022284	1399.027083	16.991693
31.302070	1385.952682	16.996711
31.103944	1385.963875	17.001728
31.145047	1386.827170	17.006746
31.052878	1390.428626	17.011763
31.387296	1398.795973	17.016781
31.273331	1397.496008	17.021799
31.613369	1391.929997	17.026816
31.313710	1391.207623	17.031834
31.544623	1390.674946	17.036851
31.475352	1385.715287	17.041869
31.378009	1396.200546	17.046887
31.769348	1394.494081	17.051904
31.850188	1391.878418	17.056922
31.851436	1390.344420	17.061939
31.763350	1392.220429	17.066957
31.692587	1387.929114	17.071975
31.917299	1381.495606	17.076992
31.786947	1381.439278	17.082010
31.810880	1386.646674	17.087027
31.808844	1383.712853	17.092045
31.576992	1388.930322	17.097063
31.813330	1383.365737	17.102080
31.424083	1381.658217	17.107098
31.532593	1376.319916	17.112115
31.898481	1379.712453	17.117133
31.578920	1378.866605	17.122151
31.607884	1387.924671	17.127168
31.358876	1393.320570	17.132186
31.596600	1388.842742	17.137203
31.853811	1398.182698	17.142221
31.679289	1410.553548	17.147239
32.324424	1411.532962	17.152256
32.115513	1418.321812	17.157274
32.252517	1406.461963	17.162291
32.089924	1414.780123	17.167309
31.871925	1414.305245	17.172327
32.168260	1404.843382	17.177344
32.214994	1412.791453	17.182362
32.489071	1404.864746	17.187379
32.502011	1392.625850	17.192397
32.167769	1410.198252	17.197415
32.509579	1403.543773	17.202432
32.446241	1408.717597	17.207450
32.269725	1401.162350	17.212467
32.704446	1404.799395	17.217485
32.391929	1404.752366	17.222503
32.547234	1405.320773	17.227520
32.296251	1403.508466	17.232538
32.511928	1402.159822	17.237555
32.443236	1404.610170	17.242573
32.190358	1408.219344	17.247591
32.588818	1409.110867	17.252608
32.217431	1403.607144	17.257626
32.057684	1409.526054	17.262643
32.812111	1416.377430	17.267661
32.981403	1436.547933	17.272679
32.928182	1433.402896	17.277696
32.904123	1431.330574	17.282714
32.663047	1435.860620	17.287731
32.727258	1439.320446	17.292749
32.889001	1430.770605	17.297767
33.057776	1427.821876	17.302784
33.014114	1433.461341	17.307802
33.283975	1437.661117	17.312819
33.300314	1425.051954	17.317837
32.991684	1426.444415	17.322855
33.164499	1424.068238	17.327872
33.423948	1420.460019	17.332890
33.227615	1419.661873	17.337907
33.469323	1422.218696	17.342925
33.196649	1429.686603	17.347943
33.427751	1410.067591	17.352960
33.416200	1421.232744	17.357978
33.040804	1427.854681	17.362995
33.608537	1415.129813	17.368013
33.764184	1414.863137	17.373031
33.468780	1418.523056	17.378048
33.438244	1415.747094	17.383066
33.773412	1412.147598	17.388083
33.593196	1417.525815	17.393101
33.437082	1422.400838	17.398119
33.301631	1415.409248	17.403136
33.329718	1420.058890	17.408154
33.588373	1409.367851	17.413171
33.412286	1413.589890	17.418189
33.472906	1429.501287	17.423207
33.935375	1445.281198	17.428224
33.823897	1454.870819	17.433242
33.919748	1457.240780	17.438259
34.315695	1445.056137	17.443277
33.968734	1458.947683	17.448295
34.129632	1453.274308	17.453312
34.157620	1448.194982	17.458330
33.950483	1450.698576	17.463347
34.044553	1439.195411	17.468365
33.878661	1449.959770	17.473383
34.075043	1448.847385	17.478400
33.879727	1443.638897	17.483418
34.006430	1449.301731	17.488435
33.891048	1451.101952	17.493453
34.099899	1454.043744	17.498471
34.315848	1445.273898	17.503488
34.290860	1443.014722	17.508506
33.980251	1452.821171	17.513523
34.163558	1448.253914	17.518541
34.337682	1471.303149	17.523559
34.280392	1480.379094	17.528576
34.432523	1481.615738	17.533594
34.432512	1487.087759	17.538611
34.606885	1477.890926	17.543629
34.582871	1477.980374	17.548647
34.736267	1476.982977	17.553664
35.064172	1470.368961	17.558682
34.636419	1470.899667	17.563699
34.901796	1471.380953	17.568717
34.920610	1479.882099	17.573735
34.861595	1474.360877	17.578752
34.977714	1477.575112	17.583770
34.935893	1470.861690	17.588787
35.141036	1466.037665	17.593805
34.874595	1467.244800	17.598823
34.972828	1473.336367	17.603840
35.071805	1474.796376	17.608858
35.156193	1466.169561	17.613875
35.307520	1459.383216	17.618893
35.107595	1465.619426	17.623911
35.250376	1466.999740	17.628928
35.306528	1468.010153	17.633946
35.263315	1469.780710	17.638963
35.343282	1465.623074	17.643981
35.133694	1467.375512	17.648999
35.222721	1463.832510	17.654016
35.390431	1464.094538	17.659034
35.355024	1469.972015	17.664051
35.287723	1462.663217	17.669069
35.205350	1463.530822	17.674087
35.443565	1466.922078	17.679104
35.181265	1468.226951	17.684122
34.986166	1468.107329	17.689139
35.733981	1466.193406	17.694157
35.551931	1461.917349	17.699175
35.215304	1468.115566	17.704192
35.487423	1465.712309	17.709210
35.244279	1482.931130	17.714227
35.491293	1480.002507	17.719245
35.259611	1491.647856	17.724263
35.599290	1477.713076	17.729280
35.703695	1494.215313	17.734298
35.582030	1505.851510	17.739315
35.874765	1508.865248	17.744333
35.882696	1519.833940	17.749351
35.944162	1514.704955	17.754368
36.113644	1514.513546	17.759386
36.173549	1513.981229	17.764403
36.262379	1504.681224	17.769421
36.168919	1521.072160	17.774439
36.055223	1510.116728	17.779456
36.121957	1502.106196	17.784474
36.366459	1522.425774	17.789491
36.393810	1514.488292	17.794509
36.115034	1517.488794	17.799527
36.143445	1506.349992	17.804544
36.609046	1505.604043	17.809562
36.348991	1507.966410	17.814579
36.331291	1501.358428	17.819597
36.156665	1512.922692	17.824615
36.603392	1518.145162	17.829632
37.090071	1527.215706	17.834650
36.578523	1536.459028	17.839667
36.827484	1531.857253	17.844685
36.939585	1528.412777	17.849703
36.707749	1519.254050	17.854720
37.090963	1508.841133	17.859738
36.632645	1507.231254	17.864755
36.719908	1514.010473	17.869773
36.772090	1524.224605	17.874791
36.898328	1529.319440	17.879808
37.115545	1523.096562	17.884826
36.950285	1528.436907	17.889843
37.069215	1528.670006	17.894861
36.844428	1522.214415	17.899879
37.205153	1535.360112	17.904896
37.069635	1528.783438	17.909914
37.128266	1540.061463	17.914931
37.285754	1529.361110	17.919949
36.913522	1535.000688	17.924967
37.144749	1541.334036	17.929984
37.418038	1527.282648	17.935002
37.065136	1531.681634	17.940019
37.515876	1529.870438	17.945037
37.017130	1535.332542	17.950055
37.298012	1528.899514	17.955072
37.525552	1523.608382	17.960090
37.167748	1533.840802	17.965107
37.482028	1530.985676	17.970125
37.662315	1561.914665	17.975143
37.682239	1564.272805	17.980160
37.773646	1554.257388	17.985178
37.455455	1561.199434	17.990195
37.775306	1552.774131	17.995213
37.869206	1555.552695	18.000231
37.730518	1562.383916	18.005248
38.128063	1550.978842	18.010266
37.922985	1553.860848	18.015283
38.143611	1544.068921	18.020301
38.023905	1559.429213	18.025319
37.983600	1559.977654	18.030336
38.237663	1558.485634	18.035354
38.018805	1560.894730	18.040371
37.912165	1557.094739	18.045389
37.904775	1552.712177	18.050407
38.044469	1562.279564	18.055424
37.979928	1549.193538	18.060442
37.882059	1559.514035	18.065459
38.200988	1550.893219	18.070477
38.120343	1573.042673	18.075495
38.302816	1580.899850	18.080512
38.655644	1579.562339	18.085530
38.370959	1582.585484	18.090547
38.809539	1583.269195	18.095565
38.609860	1581.157429	18.100583
38.792915	1578.254339	18.105600
38.751412	1582.211620	18.110618
38.756857	1580.692263	18.115635
38.898440	1569.233497	18.120653
38.893182	1577.237111	18.125671
38.648569	1576.277267	18.130688
38.806092	1572.537466	18.135706
38.833643	1573.858131	18.140723
39.147341	1575.395192	18.145741
39.208382	1573.780409	18.150759
38.795453	1571.277187	18.155776
39.030387	1582.835103	18.160794
38.936684	1579.193199	18.165811
39.063432	1578.418318	18.170829
39.331022	1583.842125	18.175847
38.916943	1577.662735	18.180864
38.886254	1581.490668	18.185882
39.143864	1581.319704	18.190899
38.846906	1576.166979	18.195917
38.907943	1578.382487	18.200935
38.898154	1582.095936	18.205952
39.188259	1594.522279	18.210970
39.248143	1601.990712	18.215987
39.103282	1610.204466	18.221005
39.346827	1612.858655	18.226023
39.127091	1612.452562	18.231040
39.480575	1608.528730	18.236058
39.416767	1613.453488	18.241075
39.466974	1612.318446	18.246093
39.651931	1626.294896	18.251111
39.942889	1636.793185	18.256128
39.929662	1625.637177	18.261146
39.538008	1624.361127	18.266163
39.810051	1621.446050	18.271181
40.448549	1626.155702	18.276199
40.372081	1615.841272	18.281216
40.262896	1606.332657	18.286234
39.859004	1600.970465	18.291251
39.985269	1601.565341	18.296269
40.169602	1596.726612	18.301287
39.937472	1593.742663	18.306304
40.124453	1595.091655	18.311322
40.056733	1591.283242	18.316339
40.311950	1604.621271	18.321357
40.170207	1612.571125	18.326375
40.188005	1626.120139	18.331392
40.389635	1616.428555	18.336410
40.439353	1619.540429	18.341427
40.558759	1615.230554	18.346445
40.620910	1608.428989	18.351463
40.307702	1615.462360	18.356480
40.715320	1616.531907	18.361498
40.487868	1620.164478	18.366515
40.524684	1617.327722	18.371533
40.686137	1611.141207	18.376551
40.474044	1621.460974	18.381568
40.830054	1611.801703	18.386586
40.611341	1617.810377	18.391603
40.828807	1621.416520	18.396621
41.163520	1615.341077	18.401639
40.627442	1622.848755	18.406656
40.618473	1615.121960	18.411674
40.899090	1631.090442	18.416691
41.000553	1640.262240	18.421709
41.202410	1642.021370	18.426727
41.113081	1653.742481	18.431744
41.299036	1638.799156	18.436762
41.257395	1649.341110	18.441779
41.153017	1648.803709	18.446797
41.391277	1648.314690	18.451815
41.515161	1648.376105	18.456832
41.868178	1636.242909	18.461850
41.601146	1638.647790	18.466867
41.534580	1630.221470	18.471885
41.834948	1641.128046	18.476903
41.193570	1628.100462	18.481920
41.439794	1634.029792	18.486938
41.431570	1638.561104	18.491955
41.622498	1640.942908	18.496973
41.443993	1637.341804	18.501991
41.655820	1642.801244	18.507008
41.588801	1640.160024	18.512026
41.483035	1640.769701	18.517043
41.425455	1643.270214	18.522061
41.920023	1648.058430	18.527079
41.814713	1660.724710	18.532096
42.116679	1664.429863	18.537114
42.091673	1663.471839	18.542131
41.694803	1667.860033	18.547149
41.702750	1667.011906	18.552167
41.728554	1673.847828	18.557184
41.857773	1665.189858	18.562202
41.681830	1674.598162	18.567219
41.924438	1687.283626	18.572237
42.046588	1689.336275	18.577255
41.922424	1694.553337	18.582272
42.204131	1684.651994	18.587290
42.391749	1687.270969	18.592307
42.359560	1691.775948	18.597325
42.677117	1687.795841	18.602343
42.233609	1699.738626	18.607360
42.791951	1684.397374	18.612378
42.548623	1690.725506	18.617395
42.138533	1694.106446	18.622413
42.980858	1700.437884	18.627431
42.706141	1720.538578	18.632448
42.888962	1720.546140	18.637466
43.106625	1717.166033	18.642483
43.060273	1714.444999	18.647501
43.509596	1698.550524	18.652519
43.088582	1697.126574	18.657536
43.476970	1686.226068	18.662554
43.065631	1677.472953	18.667571
42.978165	1685.094566	18.672589
43.383461	1688.736159	18.677607
43.396502	1680.806867	18.682624
43.227974	1683.122214	18.687642
43.204176	1678.421861	18.692659
43.290960	1677.963435	18.697677
43.554441	1679.425358	18.702695
43.328242	1688.483331	18.707712
43.746324	1670.841299	18.712730
43.732078	1676.525981	18.717747
43.500605	1678.276160	18.722765
43.691740	1678.117778	18.727783
43.452048	1686.902787	18.732800
43.296478	1680.102991	18.737818
43.692705	1686.968134	18.742835
43.789317	1697.755732	18.747853
43.816023	1704.181282	18.752871
43.727443	1710.940492	18.757888
43.780465	1708.411666	18.762906
43.875217	1716.917691	18.767923
43.980829	1712.793932	18.772941
44.119401	1700.803282	18.777959
43.920950	1713.076760	18.782976
44.069865	1705.812360	18.787994
44.311545	1712.259403	18.793011
43.808218	1715.070746	18.798029
44.285609	1715.297248	18.803047
44.081117	1716.324458	18.808064
44.142180	1711.174215	18.813082
44.235368	1708.026138	18.818099
44.289147	1729.847258	18.823117
44.456853	1742.878636	18.828135
44.516679	1740.558522	18.833152
44.383758	1744.699487	18.838170
44.548564	1743.638374	18.843187
44.493445	1738.901849	18.848205
44.541857	1736.663547	18.853223
44.774571	1745.222728	18.858240
44.393105	1739.648505	18.863258
44.676989	1745.259043	18.868275
44.327515	1740.296454	18.873293
44.727645	1743.164896	18.878311
44.804737	1759.625481	18.883328
44.819197	1763.570786	18.888346
45.146493	1765.557980	18.893363
44.893505	1773.130666	18.898381
45.257531	1762.814065	18.903399
45.349109	1765.612737	18.908416
45.440857	1757.955020	18.913434
45.000175	1757.954800	18.918451
44.570365	1757.422069	18.923469
45.211277	1759.138827	18.928487
45.173967	1762.159234	18.933504
45.645389	1766.655649	18.938522
45.647561	1752.565093	18.943539
45.631170	1762.457663	18.948557
45.671738	1752.025338	18.953575
45.628438	1752.647904	18.958592
45.688396	1756.820714	18.963610
45.589027	1754.427351	18.968627
45.221028	1763.188374	18.973645
45.439311	1761.740055	18.978663
45.798864	1777.964911	18.983680
45.788838	1781.080805	18.988698
46.253913	1783.084164	18.993715
46.021327	1795.440524	18.998733
46.297153	1784.897174	19.003751
46.197109	1787.031116	19.008768
46.389901	1778.949175	19.013786
46.326592	1777.696696	19.018803
45.900558	1766.017205	19.023821
46.268808	1775.759873	19.028839
46.261504	1781.445412	19.033856
46.174601	1789.485883	19.038874
46.430585	1780.002915	19.043891
46.207494	1776.059553	19.048909
46.529216	1779.802408	19.053927
46.259971	1780.768690	19.058944
45.996708	1772.351635	19.063962
46.223433	1779.151185	19.068979
46.267467	1788.327856	19.073997
46.691754	1786.794243	19.079015
46.905854	1798.060886	19.084032
46.646029	1803.239423	19.089050
47.028132	1800.600186	19.094067
46.444446	1802.124051	19.099085
47.031524	1810.516716	19.104103
46.938212	1807.230996	19.109120
46.731701	1795.695055	19.114138
47.094498	1800.953174	19.119155
47.066613	1802.123588	19.124173
47.117424	1799.757320	19.129191
47.150688	1796.886079	19.134208
47.165989	1800.195422	19.139226
47.397069	1793.067772	19.144243
47.253660	1805.447563	19.149261
47.031749	1815.968692	19.154279
47.115253	1815.065919	19.159296
47.228643	1823.064581	19.164314
47.485477	1822.176808	19.169331
47.580003	1836.765279	19.174349
47.372533	1826.362558	19.179367
47.656102	1832.140110	19.184384
47.415848	1828.699975	19.189402
47.717913	1830.357100	19.194419
47.826967	1834.408414	19.199437
48.034946	1834.873627	19.204455
48.111818	1841.787389	19.209472
47.688489	1831.103080	19.214490
48.049149	1834.821785	19.219507
48.033463	1845.238707	19.224525
48.208540	1839.458118	19.229543
48.287963	1852.388457	19.234560
48.164916	1851.126179	19.239578
48.238838	1842.430415	19.244595
48.182179	1845.443019	19.249613
48.186862	1840.935146	19.254631
48.233826	1851.092483	19.259648
47.799826	1845.420226	19.264666
48.330933	1837.586175	19.269683
48.380654	1848.028882	19.274701
48.666297	1842.378412	19.279719
48.912086	1837.510141	19.284736
48.761715	1840.992202	19.289754
48.489470	1836.298688	19.294771
48.296767	1846.229955	19.299789
48.493112	1855.716489	19.304807
48.843660	1876.351653	19.309824
48.494869	1880.859112	19.314842
48.930808	1867.097812	19.319859
49.148591	1866.095242	19.324877
48.709417	1862.522681	19.329895
49.002754	1860.515069	19.334912
48.901916	1872.456363	19.339930
49.154246	1872.976439	19.344947
48.996939	1869.756814	19.349965
49.303374	1879.777897	19.354983
49.620469	1887.672782	19.360000
49.390206	1889.489713	19.365018
50.014930	1877.194411	19.370035
49.411179	1866.711608	19.375053
49.296230	1865.928703	19.380071
49.901112	1871.903462	19.385088
49.768429	1884.282721	19.390106
49.415121	1868.858382	19.395123
49.268638	1877.923738	19.400141
49.873041	1883.029673	19.405159
50.109820	1883.209405	19.410176
49.552467	1900.916155	19.415194
49.870033	1890.887089	19.420211
49.980938	1897.874375	19.425229
49.940421	1884.397863	19.430247
50.050014	1887.635311	19.435264
49.948672	1890.139173	19.440282
50.022627	1893.825050	19.445299
49.953312	1887.965224	19.450317
50.408586	1892.404901	19.455335
50.853929	1905.837694	19.460352
50.789616	1894.628927	19.465370
50.460125	1882.000671	19.470387
50.126172	1889.839185	19.475405
50.435048	1881.184811	19.480423
50.475741	1897.975984	19.485440
50.204581	1915.538116	19.490458
50.506999	1918.263320	19.495475
50.359172	1916.931909	19.500493
50.501153	1914.127687	19.505511
51.023519	1916.362133	19.510528
50.663407	1914.429643	19.515546
50.994122	1907.429933	19.520563
50.843120	1916.965752	19.525581
50.741718	1919.879083	19.530599
51.214800	1929.532441	19.535616
51.250384	1935.259755	19.540634
51.363415	1938.069472	19.545651
51.502849	1934.024701	19.550669
51.455216	1926.549433	19.555687
51.698893	1926.162267	19.560704
51.459242	1910.961196	19.565722
51.447922	1899.783414	19.570739
51.674739	1898.804150	19.575757
51.377064	1890.240364	19.580775
51.568680	1901.160800	19.585792
51.796574	1919.906855	19.590810
52.055357	1924.363329	19.595827
51.930877	1918.574044	19.600845
51.892903	1903.156512	19.605863
52.043707	1901.646126	19.610880
51.487302	1897.826428	19.615898
51.630127	1899.481582	19.620915
51.712524	1921.295870	19.625933
51.886550	1925.080934	19.630951
52.053776	1926.739138	19.635968
51.935648	1927.582372	19.640986
52.245398	1917.927030	19.646003
52.112729	1927.733446	19.651021
52.450196	1935.050564	19.656039
52.495905	1920.974692	19.661056
52.353671	1923.278634	19.666074
52.430274	1923.592372	19.671091
52.506337	1925.999147	19.676109
52.500856	1928.285171	19.681127
52.329798	1921.670906	19.686144
52.300692	1929.470380	19.691162
52.646117	1935.569231	19.696179
52.698883	1957.336900	19.701197
52.841713	1955.160100	19.706215
53.128128	1947.396040	19.711232
52.905004	1964.206558	19.716250
52.686807	1954.746488	19.721267
52.982446	1957.867711	19.726285
52.826795	1953.407221	19.731303
52.928767	1951.938774	19.736320
52.731479	1951.916362	19.741338
53.019050	1951.644370	19.746355
53.290642	1967.294216	19.751373
53.210611	1982.449533	19.756391
53.542982	1981.872873	19.761408
53.268141	1983.012931	19.766426
53.188455	1982.344655	19.771443
53.443629	1981.755187	19.776461
53.345720	1985.747108	19.781479
53.731189	1990.143646	19.786496
53.495335	1995.003704	19.791514
53.436432	1981.972286	19.796531
53.405476	1987.794891	19.801549
53.746372	2008.725536	19.806567
53.703040	2005.888595	19.811584
53.974686	2009.028368	19.816602
54.049577	2007.154942	19.821619
54.078873	2001.053938	19.826637
54.151444	2013.534355	19.831655
54.418784	2002.799739	19.836672
54.156312	2017.707734	19.841690
54.562924	1993.578513	19.846707
54.300922	2000.761454	19.851725
54.636452	2007.514347	19.856743
54.791501	1994.477415	19.861760
54.589424	2005.532800	19.866778
54.677365	2002.056392	19.871795
54.718605	1995.389620	19.876813
54.483172	1999.610226	19.881831
54.486512	1996.817921	19.886848
54.595287	2007.992706	19.891866
54.786721	2011.863494	19.896883
55.040437	2021.135114	19.901901
54.955762	2018.782191	19.906919
55.002491	2014.954723	19.911936
55.240771	2022.752883	19.916954
55.175456	2018.478996	19.921971
55.035895	2025.336155	19.926989
54.951940	2020.297226	19.932007
55.492040	2017.358951	19.937024
55.058107	2020.800208	19.942042
55.334710	2014.519662	19.947059
55.358064	2010.092116	19.952077
55.529329	2016.153693	19.957095
55.451490	2014.916593	19.962112
55.479808	2025.917702	19.967130
55.444930	2015.050438	19.972147
55.404208	2024.831454	19.977165
55.399697	2035.529336	19.982183
56.120748	2042.747950	19.987200
55.790632	2053.682047	19.992218
55.956410	2047.658427	19.997235
55.908641	2049.629809	20.002253
55.765029	2052.743073	20.007271
56.053050	2048.927612	20.012288
55.978275	2044.004087	20.017306
55.943481	2047.035944	20.022323
56.666364	2044.470558	20.027341
56.191483	2047.473709	20.032359
56.167178	2040.987460	20.037376
56.333424	2040.311137	20.042394
56.444153	2044.384671	20.047411
56.554086	2047.750446	20.052429
56.717503	2068.255431	20.057447
56.818498	2064.445344	20.062464
56.623958	2073.958152	20.067482
56.847639	2071.368332	20.072499
56.752226	2067.751793	20.077517
56.836174	2065.545750	20.082535
56.875563	2068.058229	20.087552
56.892273	2074.015496	20.092570
56.711172	2062.848387	20.097587
57.041922	2076.212899	20.102605
56.646638	2071.451494	20.107623
56.990263	2064.670842	20.112640
56.912890	2084.721612	20.117658
57.107162	2090.352233	20.122675
57.593994	2102.789325	20.127693
57.306548	2104.529133	20.132711
57.680490	2093.573254	20.137728
57.567504	2096.818073	20.142746
57.418487	2092.500937	20.147763
57.698580	2092.731770	20.152781
57.755168	2091.500359	20.157799
57.832773	2085.517309	20.162816
57.814639	2093.586709	20.167834
57.943935	2088.016764	20.172851
57.837758	2091.464004	20.177869
57.624328	2099.634250	20.182887
58.040605	2101.673293	20.187904
58.449730	2115.507159	20.192922
58.164717	2108.138827	20.197939
58.571323	2109.532998	20.202957
58.460563	2101.436584	20.207975
58.512968	2114.829502	20.212992
58.302794	2107.865325	20.218010
58.552519	2106.936982	20.223027
58.652994	2109.335412	20.228045
58.422910	2108.311708	20.233063
58.138990	2104.707476	20.238080
58.418628	2105.949437	20.243098
58.528068	2110.701173	20.248115
58.805693	2098.419469	20.253133
58.935667	2112.860201	20.258151
59.319249	2120.454031	20.263168
59.103763	2122.811471	20.268186
58.987368	2116.877462	20.273203
59.408201	2117.436577	20.278221
59.154020	2126.147064	20.283239
59.277071	2122.072280	20.288256
58.941031	2122.209459	20.293274
59.360248	2124.898825	20.298291
59.503609	2130.531984	20.303309
59.448236	2132.866457	20.308327
59.541164	2131.719580	20.313344
59.721744	2126.543110	20.318362
59.335783	2121.671480	20.323379
59.866645	2121.276129	20.328397
59.390110	2133.466058	20.333415
59.679201	2125.808162	20.338432
59.316104	2129.007392	20.343450
59.338717	2134.625900	20.348467
59.738607	2145.881718	20.353485
59.744756	2155.090077	20.358503
59.701326	2150.167628	20.363520
59.755625	2157.185271	20.368538
59.881634	2156.598286	20.373555
60.606622	2176.369070	20.378573
60.507413	2181.050254	20.383591
60.458790	2176.027078	20.388608
60.510930	2183.447860	20.393626
60.531010	2176.967985	20.398643
60.605467	2185.319748	20.403661
60.634250	2178.721498	20.408679
60.671276	2177.804747	20.413696
61.004246	2177.298850	20.418714
60.936620	2181.941733	20.423731
61.082663	2187.019727	20.428749
61.016359	2185.516128	20.433767
60.975857	2173.924463	20.438784
60.871331	2178.054935	20.443802
60.884810	2182.852111	20.448819
61.091273	2172.888113	20.453837
60.987898	2178.143628	20.458855
61.462156	2170.441270	20.463872
61.077162	2176.529267	20.468890
61.017530	2188.185231	20.473907
61.270959	2186.431439	20.478925
61.349464	2200.762661	20.483943
61.671824	2200.078986	20.488960
61.666872	2195.825765	20.493978
61.450323	2198.513324	20.498995
61.809369	2188.146874	20.504013
61.602781	2199.967342	20.509031
61.873833	2199.883128	20.514048
61.833392	2208.599216	20.519066
62.038744	2217.851403	20.524083
62.330516	2225.901447	20.529101
62.079006	2229.283408	20.534119
62.106917	2227.513014	20.539136
61.942039	2227.138371	20.544154
62.078722	2229.187899	20.549171
62.095405	2225.624419	20.554189
62.413707	2244.797646	20.559207
62.333430	2241.830552	20.564224
62.358766	2243.005967	20.569242
62.594901	2247.695821	20.574259
62.934182	2247.196358	20.579277
62.643031	2255.493338	20.584295
62.939749	2251.587015	20.589312
62.965132	2239.304840	20.594330
63.193366	2245.128720	20.599347
63.343397	2247.355180	20.604365
62.927670	2234.338145	20.609383
63.366146	2239.738220	20.614400
63.085665	2243.979737	20.619418
62.907415	2245.057360	20.624435
63.156407	2240.467185	20.629453
63.040382	2250.225771	20.634471
63.078927	2263.263618	20.639488
63.475883	2266.227966	20.644506
63.336684	2272.207975	20.649523
63.683373	2266.225184	20.654541
63.648408	2271.107184	20.659559
63.735549	2265.342574	20.664576
63.605732	2255.195220	20.669594
63.594080	2271.930107	20.674611
64.018531	2287.427402	20.679629
64.093772	2298.100055	20.684647
64.121436	2292.561039	20.689664
64.278393	2290.033808	20.694682
64.009881	2292.395723	20.699699
64.281202	2276.928182	20.704717
64.383046	2285.226644	20.709735
64.238506	2278.577913	20.714752
64.482711	2290.487987	20.719770
64.570808	2287.101651	20.724787
64.783549	2288.352342	20.729805
64.728129	2286.929217	20.734823
64.493675	2281.039498	20.739840
65.004790	2284.130227	20.744858
64.667314	2284.832234	20.749875
65.022990	2282.767789	20.754893
65.225097	2305.868359	20.759911
65.213476	2302.474909	20.764928
65.052533	2295.496590	20.769946
65.083046	2305.404576	20.774963
65.373414	2316.227060	20.779981
65.171033	2317.204743	20.784999
65.487020	2299.412366	20.790016
65.320126	2316.431284	20.795034
65.171466	2309.010750	20.800051
65.596106	2303.188274	20.805069
65.499974	2310.535238	20.810087
65.652554	2306.672848	20.815104
65.658040	2306.048725	20.820122
65.520823	2315.079334	20.825139
66.072794	2328.632642	20.830157
65.840992	2338.802989	20.835175
65.880295	2338.581157	20.840192
65.956422	2332.612431	20.845210
65.795535	2348.818545	20.850227
65.952744	2335.391583	20.855245
66.047102	2348.021818	20.860263
66.052294	2350.392754	20.865280
66.705828	2357.656163	20.870298
66.436609	2363.951844	20.875315
66.783536	2356.661441	20.880333
66.397449	2364.706077	20.885351
66.537804	2360.240552	20.890368
66.864048	2357.512044	20.895386
66.663855	2362.503718	20.900403
66.896814	2355.437314	20.905421
66.780147	2357.877250	20.910439
67.176903	2364.663079	20.915456
67.466334	2361.291424	20.920474
66.808705	2362.853173	20.925491
67.184197	2374.763228	20.930509
67.272825	2381.731192	20.935527
67.276092	2383.831967	20.940544
67.741035	2388.995419	20.945562
67.436198	2391.875197	20.950579
67.437813	2384.684874	20.955597
67.665231	2384.103532	20.960615
67.885557	2378.329820	20.965632
67.906962	2382.595013	20.970650
67.948774	2383.672824	20.975667
67.961197	2380.826188	20.980685
68.015141	2389.342488	20.985703
67.997951	2385.459762	20.990720
68.073575	2372.923088	20.995738
67.825840	2381.729504	21.000755
67.849748	2375.507192	21.005773
68.249159	2391.344973	21.010791
68.051232	2404.695335	21.015808
68.384149	2411.624439	21.020826
68.423585	2410.564354	21.025843
68.690842	2408.276727	21.030861
68.434236	2411.077654	21.035879
68.908045	2405.999003	21.040896
68.791337	2403.397770	21.045914
68.599014	2410.169736	21.050931
69.004442	2405.736296	21.055949
68.962098	2398.525685	21.060967
68.733022	2407.428244	21.065984
69.104116	2400.188153	21.071002
69.022482	2423.818186	21.076019
69.169058	2426.505897	21.081037
69.051364	2432.411537	21.086055
69.232833	2430.047557	21.091072
69.803642	2427.191136	21.096090
69.323302	2430.121635	21.101107
69.261749	2423.644544	21.106125
69.694711	2425.948992	21.111143
69.588335	2434.788335	21.116160
69.598174	2432.987444	21.121178
69.818298	2458.126302	21.126195
69.741550	2452.994695	21.131213
69.916980	2451.176620	21.136231
70.063304	2458.710685	21.141248
70.137125	2448.268056	21.146266
70.182518	2457.309851	21.151283
70.352399	2460.392943	21.156301
70.355980	2454.367281	21.161319
69.919182	2444.876963	21.166336
70.379392	2460.728371	21.171354
70.425774	2472.415815	21.176371
70.323641	2473.231231	21.181389
70.582591	2477.798081	21.186407
70.572545	2489.550002	21.191424
70.745110	2473.901757	21.196442
70.854427	2479.809986	21.201459
70.960431	2488.188187	21.206477
70.935178	2497.159415	21.211495
70.641173	2511.672295	21.216512
71.200495	2500.724415	21.221530
71.076964	2505.589655	21.226547
71.279746	2496.439491	21.231565
71.491226	2501.205949	21.236583
71.146991	2499.059326	21.241600
71.793087	2496.901488	21.246618
71.803863	2517.271308	21.251635
71.761601	2509.297992	21.256653
72.004064	2513.664815	21.261671
72.201537	2526.905321	21.266688
72.072374	2511.610952	21.271706
72.040940	2512.733579	21.276723
71.953890	2522.254454	21.281741
72.370579	2521.809887	21.286759
72.453037	2530.799916	21.291776
72.788496	2522.733340	21.296794
72.469871	2515.250687	21.301811
72.398409	2500.513735	21.306829
72.284798	2493.854279	21.311847
72.454813	2514.269386	21.316864
72.482285	2518.587552	21.321882
72.039636	2519.866067	21.326899
72.490864	2530.528989	21.331917
72.205386	2525.422864	21.336935
72.738327	2532.776801	21.341952
72.701094	2545.555370	21.346970
72.731745	2558.125848	21.351987
73.015982	2554.987703	21.357005
73.205761	2555.022070	21.362023
73.072428	2553.378738	21.367040
72.695067	2545.948317	21.372058
72.987700	2564.516313	21.377075
73.380490	2575.104291	21.382093
73.856093	2565.736461	21.387111
73.747561	2565.404845	21.392128
73.705623	2567.778105	21.397146
73.447540	2569.297340	21.402163
73.793691	2572.131569	21.407181
73.712676	2565.811587	21.412199
73.803995	2569.344741	21.417216
73.953715	2580.665136	21.422234
74.220456	2599.257540	21.427251
74.263008	2593.797060	21.432269
74.547912	2581.363763	21.437287
74.133559	2598.418057	21.442304
74.257509	2585.026310	21.447322
74.651015	2602.184654	21.452339
74.523679	2584.438584	21.457357
74.620550	2584.661180	21.462375
74.639512	2595.498088	21.467392
74.644952	2587.292805	21.472410
74.629068	2591.633131	21.477427
74.999557	2602.542162	21.482445
75.106780	2607.482618	21.487463
74.956489	2615.272184	21.492480
75.065554	2612.640620	21.497498
75.142606	2609.100917	21.502515
75.240930	2610.630438	21.507533
75.404581	2607.539416	21.512551
75.194174	2612.051335	21.517568
75.631124	2623.321052	21.522586
75.569574	2637.875485	21.527603
75.565220	2640.683899	21.532621
75.911211	2634.203023	21.537639
76.018002	2640.436161	21.542656
76.076789	2627.275260	21.547674
75.948924	2636.788395	21.552691
75.906284	2636.079308	21.557709
76.482088	2638.760163	21.562727
76.049032	2641.426555	21.567744
76.319419	2629.633853	21.572762
76.239388	2630.429081	21.577779
76.421279	2652.622434	21.582797
76.655433	2651.736405	21.587815
76.470794	2663.109860	21.592832
77.116287	2651.057776	21.597850
76.921068	2657.739377	21.602867
76.725513	2649.947680	21.607885
76.898520	2653.724037	21.612903
76.585245	2653.105432	21.617920
77.254919	2649.684931	21.622938
77.191697	2654.657956	21.627955
77.080705	2651.037954	21.632973
77.219058	2647.069168	21.637991
77.324805	2668.275089	21.643008
77.687779	2668.584342	21.648026
77.721670	2681.030359	21.653043
77.737679	2682.951888	21.658061
77.924355	2672.713271	21.663079
77.857046	2671.446420	21.668096
77.798919	2663.598101	21.673114
78.014940	2671.380588	21.678131
77.768275	2682.687945	21.683149
77.802951	2674.817166	21.688167
77.553554	2682.930282	21.693184
77.638466	2677.048165	21.698202
78.070965	2686.782739	21.703219
78.100000	2705.310292	21.708237
78.273726	2699.073281	21.713255
78.290624	2709.848796	21.718272
78.101322	2709.477396	21.723290
78.494241	2713.511469	21.728307
78.459600	2729.373037	21.733325
78.880081	2734.686498	21.738343
78.731526	2733.783118	21.743360
79.110129	2741.339100	21.748378
79.315289	2740.076345	21.753395
79.181552	2741.267505	21.758413
79.459092	2735.540886	21.763431
78.953690	2726.351536	21.768448
79.412076	2735.123523	21.773466
79.694272	2731.906148	21.778483
79.341820	2733.575678	21.783501
79.453940	2736.202215	21.788519
79.249146	2763.763266	21.793536
79.498099	2759.906462	21.798554
79.626409	2761.913351	21.803571
79.673748	2758.447042	21.808589
79.877824	2756.595447	21.813607
79.945772	2782.475037	21.818624
80.132402	2787.930787	21.823642
80.453809	2784.919916	21.828659
80.232840	2791.079816	21.833677
80.545351	2785.608824	21.838695
80.338930	2793.316821	21.843712
80.715822	2781.474478	21.848730
80.954770	2779.710420	21.853747
80.738335	2782.824468	21.858765
80.664929	2777.086252	21.863783
80.508556	2792.169164	21.868800
81.145746	2799.416986	21.873818
81.086009	2812.496765	21.878835
81.099013	2816.741025	21.883853
81.238133	2818.946539	21.888871
81.439684	2811.361471	21.893888
81.833244	2802.322069	21.898906
81.741951	2805.512258	21.903923
81.546790	2804.765814	21.908941
81.971118	2801.072891	21.913959
81.859939	2803.150149	21.918976
81.984715	2800.629740	21.923994
82.338115	2804.301850	21.929011
81.943457	2801.369380	21.934029
82.225072	2792.982423	21.939047
82.168078	2803.181219	21.944064
82.039109	2793.319613	21.949082
82.088195	2799.641116	21.954099
82.083555	2818.823639	21.959117
82.243746	2822.259221	21.964135
82.051887	2835.637294	21.969152
82.391691	2833.768336	21.974170
82.515969	2835.829842	21.979187
82.550249	2830.790365	21.984205
82.860901	2845.995622	21.989223
82.992370	2855.651397	21.994240
83.001437	2863.629677	21.999258
83.248975	2855.231006	22.004275
83.121628	2859.807202	22.009293
83.364265	2853.732354	22.014311
83.032821	2853.527804	22.019328
83.277077	2858.072001	22.024346
83.415429	2842.316445	22.029363
83.402027	2854.688929	22.034381
83.328061	2845.014656	22.039399
83.564612	2867.928455	22.044416
83.700981	2879.406014	22.049434
83.893973	2874.272522	22.054451
83.843788	2877.023996	22.059469
84.323869	2863.783690	22.064487
84.174566	2873.251301	22.069504
84.121088	2871.428164	22.074522
84.512815	2870.913701	22.079539
84.154080	2873.161102	22.084557
84.470149	2881.438192	22.089575
84.632587	2893.587876	22.094592
84.477634	2894.400641	22.099610
84.894631	2894.174537	22.104627
84.743570	2900.886728	22.109645
85.033346	2899.588295	22.114663
84.953797	2904.109735	22.119680
85.048794	2902.716771	22.124698
84.940262	2887.710765	22.129715
84.888193	2916.587848	22.134733
85.366075	2915.611445	22.139751
85.600248	2924.278920	22.144768
85.677681	2915.706791	22.149786
85.555638	2922.444898	22.154803
85.198859	2925.870423	22.159821
85.764779	2919.664458	22.164839
85.790590	2923.951512	22.169856
85.733675	2934.347246	22.174874
86.067097	2933.232544	22.179891
85.958252	2941.015409	22.184909
86.057295	2944.652103	22.189927
86.354892	2940.434810	22.194944
85.953798	2942.138008	22.199962
86.355151	2942.348387	22.204979
86.430276	2963.414886	22.209997
86.477163	2964.462367	22.215015
86.645992	2961.512556	22.220032
86.895736	2968.907688	22.225050
87.142195	2954.182239	22.230067
87.148117	2959.275419	22.235085
87.225168	2958.296478	22.240103
87.128985	2971.760016	22.245120
87.159682	2956.848617	22.250138
87.411089	2966.507045	22.255155
87.354905	2986.953532	22.260173
87.359327	2988.261217	22.265191
87.392572	2993.081357	22.270208
87.389670	2996.240806	22.275226
87.520889	2990.978122	22.280243
87.407538	3000.167000	22.285261
87.780483	3008.675313	22.290279
88.130073	3020.051130	22.295296
88.303252	3017.845929	22.300314
88.650257	3013.694065	22.305331
88.261313	3019.934627	22.310349
88.576712	3011.704179	22.315367
88.576982	3014.520952	22.320384
88.134070	3018.045804	22.325402
88.764063	3018.707347	22.330419
88.456413	3013.359040	22.335437
88.824512	3007.532675	22.340455
88.709456	3016.434418	22.345472
88.890882	3026.601364	22.350490
89.070352	3033.037999	22.355507
88.971310	3032.341776	22.360525
89.019340	3027.513363	22.365543
89.500693	3029.583890	22.370560
89.269611	3032.877592	22.375578
89.718866	3031.615740	22.380595
89.141080	3032.902101	22.385613
89.399325	3050.376276	22.390631
89.381512	3063.056769	22.395648
89.550203	3063.508841	22.400666
89.935197	3060.781511	22.405683
89.529776	3071.579953	22.410701
90.148317	3080.992214	22.415719
90.226893	3094.601347	22.420736
90.126424	3094.471945	22.425754
90.506992	3079.961990	22.430771
90.451646	3093.079863	22.435789
90.638672	3083.925665	22.440807
90.708662	3088.865352	22.445824
90.617623	3083.374060	22.450842
90.756897	3087.271866	22.455859
90.842500	3105.856283	22.460877
91.133257	3108.187926	22.465895
91.176844	3107.223180	22.470912
91.146371	3119.319147	22.475930
91.317290	3107.789428	22.480947
91.464755	3113.625040	22.485965
91.426165	3114.107103	22.490983
91.539160	3105.537250	22.496000
91.539913	3108.259463	22.501018
91.951102	3127.700317	22.506035
91.783347	3139.291421	22.511053
92.012472	3129.161237	22.516071
92.213804	3133.403932	22.521088
92.028860	3133.418055	22.526106
92.225680	3136.845674	22.531123
92.528528	3137.121190	22.536141
92.443320	3127.575780	22.541159
92.528393	3135.487672	22.546176
92.370567	3140.323350	22.551194
92.385683	3146.789608	22.556211
92.613683	3163.549558	22.561229
92.948102	3154.569752	22.566247
93.064829	3156.605778	22.571264
92.590635	3165.745433	22.576282
93.258885	3162.985755	22.581299
93.126962	3190.424063	22.586317
93.202214	3187.711380	22.591335
93.530784	3188.870520	22.596352
93.262747	3185.976858	22.601370
93.632537	3179.837915	22.606387
93.627190	3187.656920	22.611405
93.432040	3190.699013	22.616423
94.255684	3202.454786	22.621440
93.942018	3210.988698	22.626458
94.058948	3217.181408	22.631475
94.426265	3218.936163	22.636493
94.097891	3210.220807	22.641511
94.194900	3209.295245	22.646528
94.397079	3213.214167	22.651546
94.477905	3206.521818	22.656563
94.751092	3216.673695	22.661581
95.040468	3229.397564	22.666599
95.080871	3220.506170	22.671616
95.154613	3223.271441	22.676634
95.303262	3208.187502	22.681651
94.916883	3212.751172	22.686669
95.377466	3226.550344	22.691687
95.458313	3226.202318	22.696704
95.188456	3239.133761	22.701722
95.566265	3233.602586	22.706739
95.687648	3235.921345	22.711757
95.574189	3229.641901	22.716775
95.561056	3225.985481	22.721792
95.551891	3223.968726	22.726810
95.777274	3220.471261	22.731827
95.823553	3236.789284	22.736845
96.274426	3249.364371	22.741863
96.107753	3253.571170	22.746880
95.889661	3260.442660	22.751898
96.346506	3257.273042	22.756915
96.388268	3264.814967	22.761933
96.075878	3277.466841	22.766951
96.231950	3283.338892	22.771968
96.451822	3289.786662	22.776986
96.571006	3289.699244	22.782003
97.148158	3307.341794	22.787021
97.024078	3318.748615	22.792039
97.570234	3312.259913	22.797056
97.457355	3315.941232	22.802074
97.977856	3311.979485	22.807091
97.619020	3303.176984	22.812109
97.385269	3313.365610	22.817127
97.973655	3303.791249	22.822144
97.649129	3310.913085	22.827162
98.089001	3300.628593	22.832179
97.893622	3309.110685	22.837197
97.776223	3311.350868	22.842215
98.168411	3315.287574	22.847232
97.861048	3327.332687	22.852250
98.128273	3319.107299	22.857267
98.290451	3326.252898	22.862285
98.047162	3332.719493	22.867303
98.239872	3343.660451	22.872320
98.607546	3357.003025	22.877338
98.507117	3354.254827	22.882355
98.665990	3363.857162	22.887373
98.909749	3376.840307	22.892391
99.006698	3370.909475	22.897408
99.414775	3378.196294	22.902426
99.640206	3377.822751	22.907443
99.584070	3385.119498	22.912461
99.429026	3385.411772	22.917479
99.736075	3372.008723	22.922496
99.765002	3393.577994	22.927514
99.965503	3398.776123	22.932531
100.033812	3406.586980	22.937549
99.962226	3404.134030	22.942567
100.506559	3401.059360	22.947584
100.201795	3414.580256	22.952602
100.523332	3405.691427	22.957619
100.479639	3405.294325	22.962637
100.176123	3403.531424	22.967655
100.427114	3408.112467	22.972672
100.555467	3424.106038	22.977690
100.744974	3428.745304	22.982707
101.183517	3422.719307	22.987725
101.164902	3429.279859	22.992743
101.246929	3418.220587	22.997760
101.187225	3430.285410	23.002778
101.091105	3428.018822	23.007795
101.565575	3440.891373	23.012813
101.402782	3451.327031	23.017831
101.549479	3446.862117	23.022848
101.627308	3456.510609	23.027866
101.844609	3461.764645	23.032883
101.846717	3456.056200	23.037901
101.599942	3460.782675	23.042919
101.936021	3465.574476	23.047936
101.917643	3482.616141	23.052954
102.102354	3488.467383	23.057971
102.086265	3492.476853	23.062989
102.327814	3495.425042	23.068007
102.623456	3498.357583	23.073024
102.846739	3513.998481	23.078042
102.806770	3514.972575	23.083059
103.395553	3509.287461	23.088077
103.066931	3513.354588	23.093095
103.399395	3508.641944	23.098112
103.342207	3509.241285	23.103130
103.221510	3504.356794	23.108147
103.271271	3498.824324	23.113165
103.348984	3526.505316	23.118183
103.752138	3517.993114	23.123200
103.639447	3534.455105	23.128218
103.886733	3534.454363	23.133235
104.178708	3532.744837	23.138253
104.084496	3532.048185	23.143271
104.126152	3530.825434	23.148288
104.064991	3540.952163	23.153306
104.246322	3557.665927	23.158323
105.006575	3551.405097	23.163341
104.690799	3558.003879	23.168359
104.875227	3548.983321	23.173376
104.987692	3561.954497	23.178394
104.815105	3552.789086	23.183411
104.946777	3555.470406	23.188429
105.193942	3573.829787	23.193447
105.616841	3584.509546	23.198464
105.492486	3580.063092	23.203482
105.423857	3575.038839	23.208499
105.629220	3576.386934	23.213517
105.887265	3576.032006	23.218535
106.001293	3579.939629	23.223552
105.899438	3577.112484	23.228570
106.091036	3575.403429	23.233587
105.965318	3573.340171	23.238605
106.136823	3584.859683	23.243623
106.324989	3600.467501	23.248640
106.291365	3602.986804	23.253658
106.829687	3601.716464	23.258675
106.807196	3597.888650	23.263693
106.556144	3613.548335	23.268711
107.041145	3603.154586	23.273728
106.877889	3600.892396	23.278746
106.767351	3602.929490	23.283763
106.994863	3613.765651	23.288781
107.060043	3626.961666	23.293799
107.565187	3626.543381	23.298816
107.476495	3629.278524	23.303834
107.111209	3625.115680	23.308851
108.070286	3640.619917	23.313869
107.855937	3653.275548	23.318887
108.016655	3652.444937	23.323904
108.045337	3647.924694	23.328922
108.490284	3647.527400	23.333939
108.197542	3647.594808	23.338957
108.324035	3646.009532	23.343975
108.366183	3640.216822	23.348992
108.221331	3647.055485	23.354010
108.129370	3661.437931	23.359027
108.278742	3669.190216	23.364045
108.419712	3679.148904	23.369063
108.971476	3671.234536	23.374080
108.967965	3686.795032	23.379098
109.214871	3702.049481	23.384115
109.452235	3697.643904	23.389133
109.457289	3698.632605	23.394151
109.544825	3699.319817	23.399168
109.464668	3696.455588	23.404186
109.268449	3699.494017	23.409203
109.803967	3703.125559	23.414221
109.890272	3712.692874	23.419239
110.256360	3712.536225	23.424256
110.241121	3722.271559	23.429274
110.397466	3712.126275	23.434291
110.764544	3715.573083	23.439309
110.433797	3718.693640	23.444327
110.614540	3716.222488	23.449344
110.615021	3709.154200	23.454362
110.799664	3718.628849	23.459379
110.846103	3731.844593	23.464397
110.492753	3732.224044	23.469415
110.821615	3730.759605	23.474432
110.826502	3743.799538	23.479450
111.229709	3766.481525	23.484467
111.732663	3760.154540	23.489485
111.559930	3769.055234	23.494503
111.841321	3762.676337	23.499520
111.920808	3759.298198	23.504538
111.820996	3762.298233	23.509555
112.017005	3772.092336	23.514573
112.217176	3793.754688	23.519591
112.298110	3787.866119	23.524608
112.571568	3793.508268	23.529626
112.539921	3794.304600	23.534643
112.655573	3792.889631	23.539661
112.490531	3792.049161	23.544679
112.501462	3798.164365	23.549696
112.565771	3820.973024	23.554714
112.793134	3826.945696	23.559731
113.397138	3819.934148	23.564749
112.895753	3822.994776	23.569767
113.474350	3839.172923	23.574784
113.753112	3849.537312	23.579802
113.707432	3857.246385	23.584819
113.788855	3849.342076	23.589837
113.663362	3851.712827	23.594855
113.703534	3843.175891	23.599872
113.933779	3851.480704	23.604890
113.968224	3871.072278	23.609907
114.305452	3873.841684	23.614925
114.333838	3874.235898	23.619943
114.480823	3870.306720	23.624960
114.685533	3883.184532	23.629978
114.875729	3907.210838	23.634995
115.061422	3901.073747	23.640013
115.101485	3908.328034	23.645031
115.000883	3905.187585	23.650048
115.431454	3905.875105	23.655066
115.376659	3907.625016	23.660083
115.528675	3891.929539	23.665101
115.390064	3914.811702	23.670119
115.656120	3925.937410	23.675136
115.855526	3926.445456	23.680154
115.879734	3933.488963	23.685171
116.030713	3926.061753	23.690189
116.296240	3928.105139	23.695207
116.094339	3926.029640	23.700224
116.269046	3931.757097	23.705242
116.050982	3943.967843	23.710259
116.576311	3951.909240	23.715277
116.716904	3947.783828	23.720295
116.973263	3948.095804	23.725312
116.971708	3945.705594	23.730330
116.753109	3956.813128	23.735347
116.897479	3952.067314	23.740365
117.075527	3968.676534	23.745383
117.041485	3980.753281	23.750400
117.199064	3974.488513	23.755418
117.021719	3988.775143	23.760435
117.354356	4002.655253	23.765453
117.832033	4002.768359	23.770471
117.769567	4005.935904	23.775488
118.180236	4013.829772	23.780506
118.252871	4036.145560	23.785523
118.218083	4026.075033	23.790541
118.216685	4031.099684	23.795559
118.590990	4035.102144	23.800576
118.682934	4039.641194	23.805594
118.841223	4052.709142	23.810611
119.412439	4053.638385	23.815629
119.203762	4053.851741	23.820647
119.334543	4047.059017	23.825664
119.744319	4049.297073	23.830682
119.476577	4054.501283	23.835699
119.612270	4053.021940	23.840717
119.867925	4053.768748	23.845735
119.857206	4050.595274	23.850752
119.772961	4045.946347	23.855770
119.833621	4070.143192	23.860787
120.301728	4074.563270	23.865805
119.970084	4071.678396	23.870823
120.103818	4077.950175	23.875840
120.456053	4079.365351	23.880858
120.395340	4101.241034	23.885875
120.813085	4107.990293	23.890893
120.752326	4105.381085	23.895911
120.736525	4111.502806	23.900928
121.198278	4109.927734	23.905946
121.099037	4120.663204	23.910963
121.501614	4122.018073	23.915981
121.547978	4130.250313	23.920999
121.829840	4126.688959	23.926016
122.048760	4128.893262	23.931034
121.698251	4130.033393	23.936051
122.068799	4125.390259	23.941069
122.009487	4137.170476	23.946087
121.793925	4151.318675	23.951104
122.112492	4140.932837	23.956122
122.555184	4144.967317	23.961139
122.249014	4150.354327	23.966157
122.355214	4169.967470	23.971175
122.754809	4168.190840	23.976192
123.248500	4167.341301	23.981210
122.819066	4179.005635	23.986227
122.905390	4174.843472	23.991245
122.964349	4202.258642	23.996263
123.112262	4204.907065	24.001280
123.435523	4198.573826	24.006298
123.669621	4210.307881	24.011315
123.973130	4224.657654	24.016333
123.951056	4240.282019	24.021351
123.602669	4237.245530	24.026368
124.354532	4232.032062	24.031386
123.981797	4235.909399	24.036403
124.407581	4229.535547	24.041421
124.894607	4245.488294	24.046439
124.744689	4259.024047	24.051456
124.747005	4253.638560	24.056474
125.045319	4255.454083	24.061491
125.152431	4254.872515	24.066509
125.284997	4243.469200	24.071527
125.216189	4253.690190	24.076544
125.448211	4239.236839	24.081562
124.852140	4246.035883	24.086579
125.483477	4268.468983	24.091597
125.937193	4271.119552	24.096615
125.968626	4275.828558	24.101632
126.039912	4264.797638	24.106650
126.221772	4274.371527	24.111667
126.086545	4276.806955	24.116685
126.337494	4291.078076	24.121703
126.258452	4306.600896	24.126720
126.706467	4299.396424	24.131738
126.181251	4307.891137	24.136755
126.583265	4305.015481	24.141773
127.086639	4313.428888	24.146791
126.873165	4322.490997	24.151808
127.601510	4329.333835	24.156826
127.377968	4334.835595	24.161843
127.674285	4331.391508	24.166861
127.720025	4344.716958	24.171879
127.818050	4355.675877	24.176896
128.035609	4354.531044	24.181914
127.922253	4359.542048	24.186931
127.799328	4357.687313	24.191949
128.206160	4369.519683	24.196967
127.875589	4393.048603	24.201984
128.267898	4376.182346	24.207002
128.253101	4388.116039	24.212019
128.287911	4408.436696	24.217037
128.868645	4418.910157	24.222055
128.873538	4424.608027	24.227072
128.978982	4420.818290	24.232090
128.980649	4438.739326	24.237107
129.538309	4444.952878	24.242125
129.639356	4445.592997	24.247143
129.512722	4439.150651	24.252160
130.063847	4457.820257	24.257178
130.210070	4473.244518	24.262195
130.015191	4464.649294	24.267213
130.617792	4462.090069	24.272231
130.236335	4469.594751	24.277248
130.437709	4466.510510	24.282266
130.440608	4472.041768	24.287283
130.568667	4484.692172	24.292301
131.250304	4490.260695	24.297319
131.047374	4505.022979	24.302336
131.399567	4491.868638	24.307354
131.336285	4491.483020	24.312371
131.414235	4493.317730	24.317389
132.195411	4507.840693	24.322407
131.957439	4515.106642	24.327424
132.231139	4509.269762	24.332442
132.356757	4508.401605	24.337459
132.519054	4509.678159	24.342477
132.509383	4506.191765	24.347495
132.402357	4513.405318	24.352512
132.618854	4501.123984	24.357530
132.554160	4509.254317	24.362547
132.625265	4513.489812	24.367565
132.897595	4502.395513	24.372583
132.662904	4518.720044	24.377600
132.667619	4518.948478	24.382618
132.684756	4520.445165	24.387635
132.725088	4533.357422	24.392653
133.177966	4541.454058	24.397671
133.035115	4560.534802	24.402688
133.582692	4560.999403	24.407706
133.705225	4575.329058	24.412723
133.541698	4584.599623	24.417741
133.771890	4582.502899	24.422759
134.169152	4603.118196	24.427776
134.385022	4612.199955	24.432794
134.438611	4620.970729	24.437811
134.585805	4612.925201	24.442829
134.920201	4611.120728	24.447847
134.864757	4618.628997	24.452864
135.239062	4630.659900	24.457882
135.472183	4639.117441	24.462899
135.099262	4643.239836	24.467917
135.432123	4634.196445	24.472935
135.633793	4646.937174	24.477952
135.775840	4644.777856	24.482970
135.706205	4665.494163	24.487987
136.008568	4670.770359	24.493005
136.277272	4669.644601	24.498023
136.193484	4670.985538	24.503040
136.517895	4677.298443	24.508058
136.661439	4694.557576	24.513075
136.719265	4697.868369	24.518093
137.095846	4680.945325	24.523111
136.648261	4692.951690	24.528128
137.442234	4709.808608	24.533146
137.422275	4716.807013	24.538163
137.488066	4720.486642	24.543181
137.794909	4719.935782	24.548199
137.624793	4722.918893	24.553216
137.896083	4709.586389	24.558234
137.923831	4723.390822	24.563251
137.575158	4744.022697	24.568269
138.261897	4746.688323	24.573287
138.047719	4744.358003	24.578304
138.467963	4752.171906	24.583322
138.557700	4765.811752	24.588339
138.638860	4781.922813	24.593357
138.671300	4772.991298	24.598375
138.676371	4792.453425	24.603392
138.971793	4798.048988	24.608410
139.296388	4801.221128	24.613427
139.261179	4810.597378	24.618445
139.571853	4822.744497	24.623463
139.583162	4836.580891	24.628480
139.758245	4827.106727	24.633498
140.063935	4840.428938	24.638515
140.349426	4854.698003	24.643533
140.625157	4852.501560	24.648551
140.747873	4861.461063	24.653568
140.681410	4853.768962	24.658586
140.792909	4859.951804	24.663603
140.745173	4863.430532	24.668621
141.242714	4871.180506	24.673639
141.082577	4881.999821	24.678656
141.156101	4881.618320	24.683674
141.588561	4883.692869	24.688691
141.537524	4889.622260	24.693709
142.051733	4898.590212	24.698727
142.037301	4912.203328	24.703744
141.719374	4910.793496	24.708762
142.292689	4911.212895	24.713779
142.108951	4916.649199	24.718797
142.538481	4904.670147	24.723815
142.405902	4930.500641	24.728832
142.665259	4938.768135	24.733850
142.680971	4942.744357	24.738867
142.804623	4941.996212	24.743885
142.951637	4937.742682	24.748903
142.982027	4949.138499	24.753920
143.267327	4957.326101	24.758938
143.425334	4966.394806	24.763955
143.583913	4961.203724	24.768973
143.920822	4973.796318	24.773991
143.533609	4981.047810	24.779008
143.854781	4997.393428	24.784026
144.493141	4992.394614	24.789043
144.271660	5004.626041	24.794061
144.618184	5019.875126	24.799079
144.790973	5015.797661	24.804096
144.510522	5014.684041	24.809114
144.922340	5025.404822	24.814131
144.792520	5043.224667	24.819149
145.517237	5039.421251	24.824167
145.149312	5058.583177	24.829184
145.485772	5050.493491	24.834202
145.774038	5052.918779	24.839219
145.830881	5062.825726	24.844237
145.978154	5059.777893	24.849255
145.796191	5066.346483	24.854272
146.517807	5087.339518	24.859290
146.831280	5091.121567	24.864307
146.722458	5113.163348	24.869325
146.894097	5095.523233	24.874343
146.677179	5106.576560	24.879360
146.592047	5109.946549	24.884378
146.917709	5115.990074	24.889395
146.877297	5127.186672	24.894413
147.334289	5133.892865	24.899431
147.366237	5163.021646	24.904448
147.776827	5164.131923	24.909466
147.890341	5154.511816	24.914483
147.995032	5175.162915	24.919501
148.370147	5175.488338	24.924519
148.305777	5175.146199	24.929536
148.248132	5177.690207	24.934554
148.811515	5195.423022	24.939571
148.356896	5208.791090	24.944589
148.912822	5212.310143	24.949607
149.015234	5218.555274	24.954624
149.199644	5229.088596	24.959642
149.644063	5232.847424	24.964659
149.335126	5237.249208	24.969677
149.711361	5224.402948	24.974695
149.847305	5253.514678	24.979712
150.220684	5259.666134	24.984730
150.435698	5259.552605	24.989747
149.960900	5265.853151	24.994765
150.678028	5265.609237	24.999783
150.800723	5282.584999	25.004800
150.914039	5285.704797	25.009818
151.155356	5283.373804	25.014835
150.951358	5287.599923	25.019853
151.063367	5279.945010	25.024871
151.129185	5304.639866	25.029888
151.309966	5321.314647	25.034906
151.568097	5315.992767	25.039923
151.838086	5326.193015	25.044941
151.757216	5341.599019	25.049959
151.720949	5347.151245	25.054976
152.096882	5343.858365	25.059994
152.116074	5347.986117	25.065011
152.279184	5364.804848	25.070029
152.613206	5378.611130	25.075047
153.004681	5370.908330	25.080064
153.112068	5376.317069	25.085082
153.453452	5373.390619	25.090099
153.061140	5387.855870	25.095117
153.451137	5387.496783	25.100135
153.504058	5388.360709	25.105152
153.801498	5384.402702	25.110170
153.881827	5400.668901	25.115187
153.725855	5423.818396	25.120205
154.100573	5427.635279	25.125223
154.079754	5427.323729	25.130240
154.156612	5444.544319	25.135258
154.656536	5441.249794	25.140275
154.641521	5455.106053	25.145293
154.925360	5466.016869	25.150311
155.340664	5477.395023	25.155328
155.246612	5473.860952	25.160346
155.481857	5475.475989	25.165363
155.303425	5485.929363	25.170381
155.680505	5496.538867	25.175399
155.796127	5499.997779	25.180416
155.947169	5506.083755	25.185434
156.359527	5520.495454	25.190451
156.313927	5532.053916	25.195469
156.334822	5534.718083	25.200487
156.884545	5538.427260	25.205504
156.972527	5549.639130	25.210522
157.204192	5561.148560	25.215539
157.197653	5569.816403	25.220557
157.292951	5560.377062	25.225575
157.542926	5557.060100	25.230592
157.536138	5579.980350	25.235610
158.010968	5585.380310	25.240627
158.161600	5592.090165	25.245645
158.053786	5592.820043	25.250663
158.471671	5606.678799	25.255680
158.439213	5618.577754	25.260698
158.567966	5616.337020	25.265715
158.736622	5615.513661	25.270733
158.880502	5629.583985	25.275751
159.037450	5650.647634	25.280768
159.256759	5647.710628	25.285786
159.095094	5646.786797	25.290803
159.287951	5670.055323	25.295821
159.486662	5679.351619	25.300839
159.656018	5682.890674	25.305856
159.834732	5709.249005	25.310874
160.283273	5705.052463	25.315891
160.465167	5712.241570	25.320909
160.409637	5716.039969	25.325927
160.589531	5729.129364	25.330944
160.638303	5738.994754	25.335962
161.043963	5738.853598	25.340979
161.267003	5746.055599	25.345997
161.483642	5760.884273	25.351015
161.391352	5762.967848	25.356032
161.985462	5774.562348	25.361050
162.195577	5761.481671	25.366067
161.937412	5770.412600	25.371085
162.606024	5780.284874	25.376103
162.550885	5791.941194	25.381120
162.452038	5797.899318	25.386138
163.020804	5786.818841	25.391155
162.845394	5792.681736	25.396173
162.899377	5788.113372	25.401191
162.914903	5800.031299	25.406208
163.024679	5814.428778	25.411226
163.301422	5813.626107	25.416243
163.020050	5824.067606	25.421261
163.303603	5829.852168	25.426279
163.722351	5838.118164	25.431296
163.739438	5846.713725	25.436314
164.076956	5854.461541	25.441331
164.239102	5868.932311	25.446349
164.062167	5871.362286	25.451367
164.344461	5888.465862	25.456384
164.535035	5902.764195	25.461402
165.016886	5894.524780	25.466419
165.074164	5923.878391	25.471437
165.159658	5935.677720	25.476455
165.241726	5936.402169	25.481472
165.582383	5946.575367	25.486490
165.706980	5956.221984	25.491507
165.621214	5957.029352	25.496525
165.560942	5972.634190	25.501543
166.105475	5987.761645	25.506560
166.143791	5994.175219	25.511578
166.739624	6005.418328	25.516595
166.866552	6017.594429	25.521613
166.813196	6022.241595	25.526631
166.992590	6026.850230	25.531648
167.640612	6040.679145	25.536666
167.895476	6046.404739	25.541683
167.786553	6046.891445	25.546701
168.090049	6036.985736	25.551719
168.299429	6058.520910	25.556736
168.416819	6070.159897	25.561754
168.776492	6071.625228	25.566771
168.874291	6070.366207	25.571789
168.725773	6071.037472	25.576807
169.047960	6071.409487	25.581824
169.471105	6094.245915	25.586842
169.617413	6093.329354	25.591859
169.342368	6094.806828	25.596877
169.380115	6091.398084	25.601895
169.616190	6110.923619	25.606912
169.383513	6127.788998	25.611930
169.528638	6124.997296	25.616947
169.889018	6151.071885	25.621965
170.171223	6156.525200	25.626983
170.374592	6166.120310	25.632000
170.504840	6186.030493	25.637018
170.928905	6182.758617	25.642035
171.139112	6203.685015	25.647053
171.133806	6216.704659	25.652071
171.596134	6219.257266	25.657088
171.706471	6226.115048	25.662106
171.783400	6237.341838	25.667123
172.142168	6255.341290	25.672141
172.112962	6256.886772	25.677159
172.337552	6251.876522	25.682176
172.592934	6271.342351	25.687194
172.776959	6267.189456	25.692212
173.085342	6283.065948	25.697229
173.069237	6280.072497	25.702247
173.383983	6281.843011	25.707264
173.242998	6294.540198	25.712282
173.523866	6296.923588	25.717300
173.466137	6297.348267	25.722317
173.560943	6304.136980	25.727335
173.647513	6324.999730	25.732352
174.111953	6333.292292	25.737370
174.221403	6339.424071	25.742388
174.290851	6361.987059	25.747405
174.364491	6367.035475	25.752423
174.354871	6358.522751	25.757440
174.876716	6392.599391	25.762458
174.778064	6389.479386	25.767476
175.377387	6403.615986	25.772493
175.337115	6417.622194	25.777511
175.949889	6409.627851	25.782528
175.598756	6414.412645	25.787546
176.141119	6422.989294	25.792564
176.228168	6436.429394	25.797581
176.384154	6447.812588	25.802599
176.704578	6445.295838	25.807616
176.727083	6471.363093	25.812634
176.953793	6469.368308	25.817652
177.240560	6468.407207	25.822669
177.294485	6480.042038	25.827687
177.771596	6485.899555	25.832704
177.556336	6505.864977	25.837722
177.873595	6507.827287	25.842740
177.798374	6507.160829	25.847757
177.985299	6525.099247	25.852775
178.090796	6524.464306	25.857792
178.217726	6541.117786	25.862810
178.662097	6554.001037	25.867828
179.068417	6559.785236	25.872845
178.828548	6563.763220	25.877863
179.425828	6586.599886	25.882880
179.429306	6588.704733	25.887898
179.471896	6588.008529	25.892916
179.978907	6610.775897	25.897933
179.940255	6616.424268	25.902951
180.492008	6612.550669	25.907968
180.475800	6622.792049	25.912986
180.765625	6640.970337	25.918004
180.909403	6642.784950	25.923021
180.661369	6646.053058	25.928039
181.230550	6656.926912	25.933056
181.350000	6681.089674	25.938074
181.203344	6676.053324	25.943092
181.633974	6684.567486	25.948109
181.633241	6707.087448	25.953127
181.804780	6714.372459	25.958144
181.969344	6728.237121	25.963162
182.275440	6738.832436	25.968180
182.486951	6740.101816	25.973197
182.532895	6754.581608	25.978215
183.368995	6758.987219	25.983232
183.249884	6763.411554	25.988250
183.546703	6761.591013	25.993268
183.681630	6770.121882	25.998285
183.745628	6791.060659	26.003303
183.898849	6800.582541	26.008320
183.735977	6799.378433	26.013338
184.146430	6808.009425	26.018356
184.447629	6827.146988	26.023373
184.560653	6828.194807	26.028391
184.742305	6834.993788	26.033408
184.772109	6855.267223	26.038426
184.707885	6860.583583	26.043444
185.434523	6869.764038	26.048461
185.190495	6889.281010	26.053479
185.985333	6881.898238	26.058496
185.754474	6903.472786	26.063514
186.027403	6912.655125	26.068532
186.154369	6909.804855	26.073549
186.124983	6923.263068	26.078567
186.729934	6930.051874	26.083584
186.667510	6939.339370	26.088602
186.882493	6939.024197	26.093620
187.066666	6943.922171	26.098637
187.202904	6964.826375	26.103655
187.761111	6957.591440	26.108672
187.676860	6973.472190	26.113690
187.592599	6980.913095	26.118708
187.886401	6983.036882	26.123725
188.034259	6998.617724	26.128743
188.071963	7008.359711	26.133760
188.296088	7033.273657	26.138778
188.521541	7039.110030	26.143796
188.952533	7052.210150	26.148813
188.784646	7065.454323	26.153831
189.177352	7072.602850	26.158848
189.486477	7088.838420	26.163866
189.692924	7086.948524	26.168884
190.232942	7099.149228	26.173901
189.777363	7109.496742	26.178919
190.144440	7117.998030	26.183936
190.363609	7127.777000	26.188954
190.813177	7146.073566	26.193972
191.180899	7144.190834	26.198989
190.951429	7153.601418	26.204007
191.088849	7157.726611	26.209024
191.223650	7176.507756	26.214042
191.621851	7188.579198	26.219060
191.601635	7203.613849	26.224077
191.739689	7209.013414	26.229095
192.029259	7217.559882	26.234112
192.159773	7217.475300	26.239130
192.599341	7238.332011	26.244148
193.000844	7252.104345	26.249165
192.866824	7257.893185	26.254183
192.977120	7265.952639	26.259200
193.602170	7272.474394	26.264218
193.554429	7275.939473	26.269236
193.890348	7284.768172	26.274253
193.972195	7302.755584	26.279271
194.375978	7321.053631	26.284288
194.502832	7326.996230	26.289306
194.831937	7337.538513	26.294324
195.351495	7340.570198	26.299341
195.228414	7344.456574	26.304359
195.331198	7337.901019	26.309376
195.569989	7349.543692	26.314394
195.621133	7368.114423	26.319412
195.756556	7371.282963	26.324429
195.916490	7381.019908	26.329447
196.167089	7388.330737	26.334464
196.062918	7391.798094	26.339482
196.216356	7412.175440	26.344500
196.710777	7429.214058	26.349517
196.557929	7441.034273	26.354535
197.153436	7459.001417	26.359552
197.456310	7467.503282	26.364570
197.191396	7478.923026	26.369588
197.596404	7482.457346	26.374605
197.602427	7496.019670	26.379623
198.250761	7518.332504	26.384640
198.362761	7525.730145	26.389658
198.587466	7523.947453	26.394676
198.725786	7537.086975	26.399693
198.867568	7557.423112	26.404711
199.226406	7559.298328	26.409728
199.384606	7556.991797	26.414746
199.366122	7582.802994	26.419764
199.768503	7582.349660	26.424781
199.950751	7587.474221	26.429799
199.547374	7590.627238	26.434816
199.916365	7609.500883	26.439834
200.068737	7617.302274	26.444852
200.487133	7626.085214	26.449869
200.531084	7651.090609	26.454887
200.770116	7665.410869	26.459904
201.239812	7679.416473	26.464922
201.259405	7682.946113	26.469940
201.513733	7699.293780	26.474957
201.489205	7702.358895	26.479975
201.760484	7715.834958	26.484992
202.374534	7738.116755	26.490010
202.269334	7748.879299	26.495028
202.508543	7752.567161	26.500045
202.599591	7767.628036	26.505063
203.030002	7775.124320	26.510080
203.174087	7787.989760	26.515098
203.086286	7806.365809	26.520116
203.673758	7808.308758	26.525133
203.722519	7819.647671	26.530151
203.927632	7829.377412	26.535168
204.114960	7843.720571	26.540186
204.056874	7861.259941	26.545204
204.478505	7863.880214	26.550221
204.852730	7889.836427	26.555239
204.996191	7898.066372	26.560256
205.148587	7915.729287	26.565274
205.454741	7921.836992	26.570292
205.795398	7936.763754	26.575309
206.255347	7951.681811	26.580327
206.642516	7937.932777	26.585344
206.645328	7950.778412	26.590362
206.851807	7963.228778	26.595380
207.444634	7972.231165	26.600397
207.096911	7975.259248	26.605415
207.433872	7975.850220	26.610432
207.572907	7988.078607	26.615450
207.625051	7993.336693	26.620468
208.027965	7996.094787	26.625485
207.871964	8009.487442	26.630503
207.753746	8032.311518	26.635520
208.522724	8044.335623	26.640538
208.317944	8066.390297	26.645556
208.695872	8066.330135	26.650573
209.194624	8083.565670	26.655591
209.015465	8101.416016	26.660608
209.379054	8111.917658	26.665626
209.235062	8128.649160	26.670644
209.804698	8136.592052	26.675661
210.062014	8152.901093	26.680679
210.070216	8170.659844	26.685696
210.567448	8173.294437	26.690714
210.586473	8189.171903	26.695732
210.991035	8183.063888	26.700749
211.274354	8208.951384	26.705767
211.272631	8221.329289	26.710784
211.605378	8227.841540	26.715802
211.606729	8247.367601	26.720820
211.801375	8246.329486	26.725837
212.335757	8270.691436	26.730855
212.335964	8279.029579	26.735872
212.667956	8287.326193	26.740890
212.717466	8305.510722	26.745908
212.923128	8318.413660	26.750925
213.579680	8326.772362	26.755943
213.498422	8341.450319	26.760960
213.689762	8343.351784	26.765978
213.829181	8349.582572	26.770996
213.939232	8363.141016	26.776013
214.061559	8374.688710	26.781031
213.968115	8393.792661	26.786048
214.630190	8402.403352	26.791066
214.505812	8426.101036	26.796084
214.777916	8429.746587	26.801101
214.996760	8448.045826	26.806119
215.097769	8462.862297	26.811136
215.695968	8473.342670	26.816154
215.830302	8494.141277	26.821172
216.587424	8498.820420	26.826189
216.631037	8503.767353	26.831207
216.511137	8522.273213	26.836224
216.930465	8530.824117	26.841242
217.074395	8538.678561	26.846260
217.397270	8546.445880	26.851277
217.798122	8564.808864	26.856295
217.781095	8559.217151	26.861312
217.942230	8580.886619	26.866330
218.183958	8588.609887	26.871348
218.405702	8596.937517	26.876365
218.622429	8618.292975	26.881383
218.566508	8620.740353	26.886400
219.216830	8636.817826	26.891418
219.318245	8653.416296	26.896436
219.420734	8657.539784	26.901453
219.682563	8669.267050	26.906471
219.547229	8683.874709	26.911488
219.879324	8703.365479	26.916506
219.841746	8716.467345	26.921524
220.331979	8728.635010	26.926541
220.568457	8745.591701	26.931559
220.654371	8763.503675	26.936576
220.984980	8783.972395	26.941594
221.138736	8795.928763	26.946612
221.195093	8821.133238	26.951629
221.930402	8831.461171	26.956647
221.794832	8840.360911	26.961664
222.589758	8865.815014	26.966682
222.566153	8869.232327	26.971700
223.441655	8892.418563	26.976717
223.410332	8907.529130	26.981735
223.353870	8904.892421	26.986752
224.041274	8914.110504	26.991770
224.227255	8931.967500	26.996788
224.505416	8929.332900	27.001805
224.225435	8934.480846	27.006823
224.287475	8943.577958	27.011840
224.762418	8959.149110	27.016858
224.689210	8968.163852	27.021876
224.936824	8989.159409	27.026893
225.631967	8995.916063	27.031911
225.522182	9023.495906	27.036928
225.950137	9024.275102	27.041946
226.209847	9036.039226	27.046964
226.413524	9039.214132	27.051981
226.487309	9052.374250	27.056999
226.667444	9052.768289	27.062016
226.734822	9077.710591	27.067034
227.057209	9086.565380	27.072052
227.460367	9104.183371	27.077069
227.654851	9112.672551	27.082087
227.427327	9124.803359	27.087104
228.126877	9139.415812	27.092122
227.939325	9150.012528	27.097140
228.422878	9163.721732	27.102157
228.628883	9163.531689	27.107175
228.725064	9175.785411	27.112192
229.098847	9178.089264	27.117210
229.179572	9187.597003	27.122228
229.693222	9205.009325	27.127245
229.730706	9219.726723	27.132263
230.121341	9219.951999	27.137280
230.631295	9242.970015	27.142298
230.380815	9263.551299	27.147316
231.026480	9270.165008	27.152333
230.960713	9278.431088	27.157351
230.924979	9286.023375	27.162368
231.379968	9292.930202	27.167386
231.400362	9315.832420	27.172404
231.820600	9321.787856	27.177421
232.003073	9338.431913	27.182439
232.156440	9358.492701	27.187456
232.364547	9361.188753	27.192474
232.118245	9387.083113	27.197492
232.797800	9403.303839	27.202509
232.991998	9429.308113	27.207527
232.936876	9449.045084	27.212544
233.370521	9468.196983	27.217562
233.546269	9484.504343	27.222580
234.158294	9504.134881	27.227597
234.334318	9514.919017	27.232615
234.301835	9525.881843	27.237632
234.995690	9541.511073	27.242650
235.155115	9556.864827	27.247668
235.675271	9576.095494	27.252685
235.713740	9577.038458	27.257703
236.121054	9585.200385	27.262720
236.263769	9604.814989	27.267738
236.391296	9605.320953	27.272756
236.461872	9624.307831	27.277773
237.142419	9628.045970	27.282791
236.970626	9649.370218	27.287808
237.419452	9657.502464	27.292826
237.314511	9673.107284	27.297844
237.725487	9688.969407	27.302861
237.940512	9704.169143	27.307879
238.341238	9719.767504	27.312896
238.670255	9719.251426	27.317914
238.904334	9737.172260	27.322932
239.537690	9749.084611	27.327949
239.600562	9754.378528	27.332967
239.514478	9763.587283	27.337984
240.091983	9771.892874	27.343002
240.155268	9786.295338	27.348020
240.088988	9789.110150	27.353037
240.619749	9822.452120	27.358055
240.734245	9824.518532	27.363072
241.010056	9831.228366	27.368090
241.141028	9850.453673	27.373108
241.065612	9865.036729	27.378125
241.758866	9871.089771	27.383143
241.665034	9896.343643	27.388160
242.104692	9910.249830	27.393178
242.478391	9923.256236	27.398196
242.177691	9941.881106	27.403213
242.597944	9948.493024	27.408231
242.346862	9973.790380	27.413248
243.242786	9982.790220	27.418266
243.392576	9999.192998	27.423284
243.622682	10024.103529	27.428301
243.951428	10034.065463	27.433319
244.220786	10049.444032	27.438336
244.423102	10063.809548	27.443354
244.879632	10071.787894	27.448372
244.858807	10087.900727	27.453389
245.380375	10095.625670	27.458407
245.177028	10105.233761	27.463424
245.816786	10122.161392	27.468442
246.342146	10123.349161	27.473460
246.803841	10130.211125	27.478477
247.161709	10145.680703	27.483495
246.957429	10156.061046	27.488512
247.302394	10141.298466	27.493530
247.047821	10152.886987	27.498548
247.437845	10173.406734	27.503565
247.762289	10167.559404	27.508583
247.897171	10193.633821	27.513600
248.496971	10204.902901	27.518618
248.568561	10212.789838	27.523636
248.744253	10234.792381	27.528653
248.836115	10242.120558	27.533671
248.832774	10255.995597	27.538688
249.250933	10274.103211	27.543706
249.098029	10294.395492	27.548724
249.525678	10320.464194	27.553741
249.854665	10334.704991	27.558759
250.013615	10357.025606	27.563776
250.482809	10370.571990	27.568794
250.583260	10387.704989	27.573812
250.930326	10415.883615	27.578829
251.404512	10425.541247	27.583847
251.302769	10445.702346	27.588864
251.770738	10460.472522	27.593882
252.172186	10483.486648	27.598900
252.423433	10497.766457	27.603917
252.896510	10512.460202	27.608935
252.683775	10522.237905	27.613952
253.051767	10528.131537	27.618970
253.471559	10558.461001	27.623988
253.758239	10561.821796	27.629005
254.151873	10578.013050	27.634023
254.309128	10595.409460	27.639040
254.867309	10604.511258	27.644058
255.063987	10618.024967	27.649076
254.885977	10616.990880	27.654093
255.763964	10623.591124	27.659111
255.842725	10643.116736	27.664128
256.239267	10647.890095	27.669146
256.602990	10662.657229	27.674164
256.695879	10673.544145	27.679181
256.782347	10669.584322	27.684199
257.138131	10694.148918	27.689216
257.319626	10697.799749	27.694234
257.372407	10709.298398	27.699252
257.440918	10731.589595	27.704269
257.976754	10740.575416	27.709287
257.813373	10765.720832	27.714304
257.768573	10778.745210	27.719322
258.465084	10792.256686	27.724340
258.511952	10808.406305	27.729357
259.255930	10827.554153	27.734375
259.186824	10855.703169	27.739392
259.544836	10870.677859	27.744410
260.174108	10886.984839	27.749428
260.206024	10899.620019	27.754445
260.621099	10914.306401	27.759463
260.664579	10924.421683	27.764480
261.140452	10940.820291	27.769498
261.424229	10953.864479	27.774516
261.306069	10971.443973	27.779533
261.630935	10984.467203	27.784551
261.672946	10998.563065	27.789568
261.728176	11009.224809	27.794586
262.489697	11030.858076	27.799604
262.680431	11052.114711	27.804621
263.250544	11049.883681	27.809639
263.306349	11068.132534	27.814656
263.618855	11077.068848	27.819674
264.089844	11076.146327	27.824692
264.223365	11105.901005	27.829709
264.904523	11099.950172	27.834727
264.552711	11119.361697	27.839744
264.811169	11121.309115	27.844762
265.134358	11132.734940	27.849780
264.984079	11163.709055	27.854797
265.255277	11169.653614	27.859815
265.378227	11196.436774	27.864832
266.285486	11208.399421	27.869850
266.231570	11233.956047	27.874868
266.453261	11243.263607	27.879885
266.938065	11266.263478	27.884903
267.141477	11276.138203	27.889920
267.138340	11294.332463	27.894938
267.601252	11319.866703	27.899956
267.660786	11342.043622	27.904973
268.198050	11346.842745	27.909991
268.222900	11379.283682	27.915008
268.494321	11390.801776	27.920026
269.090560	11415.560880	27.925044
268.927032	11436.763207	27.930061
269.459554	11442.210788	27.935079
269.731274	11471.949565	27.940096
269.774532	11491.820871	27.945114
270.349535	11505.674522	27.950132
270.714325	11528.130503	27.955149
271.001098	11548.150663	27.960167
271.209147	11555.476749	27.965184
271.572057	11575.517431	27.970202
272.185937	11580.587585	27.975220
272.269833	11619.316074	27.980237
272.699776	11618.702872	27.985255
272.951369	11629.475917	27.990272
273.392035	11646.930550	27.995290
273.985999	11648.352910	28.000308
273.734664	11658.485935	28.005325
274.369616	11673.292618	28.010343
274.392546	11682.152714	28.015360
274.533269	11692.233470	28.020378
274.749562	11697.128377	28.025396
274.948274	11723.397189	28.030413
275.267657	11740.459139	28.035431
275.315983	11754.727952	28.040448
275.512735	11778.061455	28.045466
276.260616	11787.424051	28.050484
276.418192	11807.399734	28.055501
276.575875	11816.841133	28.060519
276.759753	11840.053943	28.065536
277.111248	11862.408586	28.070554
277.178501	11875.289232	28.075572
277.447266	11893.886688	28.080589
277.858155	11895.035244	28.085607
277.900439	11928.673591	28.090624
278.321137	11951.188667	28.095642
278.918727	11967.412166	28.100660
279.042264	11979.120620	28.105677
279.062884	11995.152852	28.110695
279.719630	12008.567932	28.115712
279.870209	12028.458375	28.120730
280.594976	12019.568952	28.125748
280.666584	12045.005225	28.130765
280.847115	12050.635769	28.135783
281.243717	12056.367647	28.140800
281.524534	12072.832788	28.145818
281.805369	12081.292697	28.150836
281.748209	12101.704550	28.155853
282.108311	12106.886217	28.160871
282.328965	12129.288101	28.165888
282.224740	12142.172130	28.170906
282.618193	12155.073068	28.175924
282.580899	12173.633259	28.180941
283.492063	12203.923086	28.185959
283.479680	12215.699909	28.190976
283.596708	12226.743035	28.195994
283.951966	12256.344932	28.201012
284.357709	12280.156716	28.206029
284.549271	12296.211377	28.211047
284.863017	12315.938064	28.216064
284.631087	12345.002248	28.221082
285.131494	12365.192918	28.226100
285.509810	12387.792833	28.231117
285.792687	12413.757296	28.236135
286.222424	12432.024581	28.241152
286.622297	12459.312391	28.246170
287.020079	12476.524455	28.251188
287.323691	12506.986330	28.256205
287.887237	12507.970986	28.261223
287.890268	12532.621980	28.266240
288.125289	12552.738621	28.271258
288.704953	12569.365967	28.276276
288.684101	12600.518381	28.281293
289.041264	12610.653707	28.286311
289.726925	12639.210379	28.291328
289.624638	12649.152303	28.296346
290.204231	12662.862784	28.301364
290.221111	12692.545125	28.306381
290.689385	12703.353935	28.311399
291.088867	12717.046999	28.316416
290.928567	12741.309306	28.321434
291.381540	12755.672761	28.326452
291.375411	12780.956006	28.331469
291.673257	12792.396657	28.336487
292.223866	12830.880581	28.341504
292.600845	12848.031871	28.346522
293.035065	12861.448250	28.351540
292.892736	12888.804467	28.356557
293.337461	12900.510849	28.361575
293.955496	12939.946755	28.366592
294.313166	12953.642212	28.371610
294.978847	12967.976950	28.376628
294.957379	12985.697056	28.381645
295.387427	12999.859652	28.386663
295.753461	13009.984304	28.391680
296.139969	13032.500237	28.396698
296.517221	13032.652158	28.401716
296.552044	13051.111583	28.406733
296.886222	13067.690248	28.411751
297.224100	13070.841379	28.416768
297.579269	13087.537935	28.421786
297.726234	13095.215233	28.426804
297.775250	13124.410805	28.431821
298.113032	13143.512024	28.436839
298.030828	13155.097787	28.441856
298.054417	13173.979987	28.446874
298.684111	13194.342554	28.451892
298.871471	13220.141305	28.456909
299.740876	13239.624273	28.461927
299.855608	13259.750667	28.466944
299.890130	13281.061295	28.471962
300.174474	13294.308999	28.476980
300.471510	13304.446832	28.481997
300.930224	13313.982686	28.487015
301.204119	13338.914710	28.492032
301.044745	13364.473227	28.497050
301.832037	13371.600244	28.502068
301.549948	13404.166943	28.507085
302.233858	13422.689554	28.512103
302.504338	13448.649840	28.517120
302.420511	13467.639989	28.522138
303.398403	13488.933424	28.527156
303.181332	13513.165299	28.532173
303.732931	13533.610561	28.537191
304.372046	13544.680059	28.542208
304.420017	13583.605132	28.547226
305.082885	13590.292656	28.552244
305.237524	13615.881540	28.557261
305.295971	13628.079478	28.562279
306.055933	13638.657818	28.567296
306.103155	13658.925110	28.572314
306.662174	13679.635669	28.577332
306.902279	13699.275361	28.582349
307.061868	13714.813485	28.587367
307.474601	13731.635134	28.592384
307.758142	13757.451910	28.597402
308.172523	13761.882832	28.602420
308.355396	13781.249992	28.607437
308.566192	13801.885962	28.612455
308.901852	13815.138204	28.617472
308.813700	13845.626452	28.622490
309.395784	13862.528949	28.627508
309.893020	13893.386889	28.632525
309.934493	13915.504111	28.637543
310.288361	13929.585567	28.642560
310.369773	13953.120945	28.647578
310.940341	13978.703015	28.652596
311.264368	14003.523740	28.657613
311.285500	14036.188074	28.662631
311.765415	14046.690105	28.667648
311.964034	14087.058720	28.672666
312.542299	14095.878641	28.677684
312.962001	14126.745128	28.682701
313.426385	14158.072360	28.687719
313.912625	14164.746806	28.692736
314.220956	14188.616908	28.697754
314.575384	14207.131908	28.702772
314.697983	14222.219585	28.707789
314.752748	14243.513931	28.712807
315.169668	14249.392952	28.717824
315.519713	14280.617989	28.722842
315.945146	14298.503529	28.727860
316.297160	14314.776333	28.732877
316.052133	14337.444305	28.737895
316.570826	14350.827444	28.742912
316.926823	14383.414979	28.747930
317.426594	14401.209524	28.752948
317.793494	14418.876356	28.757965
317.497116	14446.077849	28.762983
318.200130	14473.269998	28.768000
318.271363	14502.658208	28.773018
318.669304	14521.183698	28.778036
319.141114	14543.200592	28.783053
319.573284	14571.006696	28.788071
319.820226	14594.364293	28.793088
320.041151	14615.639500	28.798106
320.538895	14631.730890	28.803124
320.662753	14651.781834	28.808141
321.148107	14678.827527	28.813159
321.604986	14689.477211	28.818176
321.826739	14718.919698	28.823194
322.133805	14726.531861	28.828212
322.326171	14750.537031	28.833229
322.648670	14766.693810	28.838247
323.337498	14774.069437	28.843264
323.245644	14806.963627	28.848282
323.225227	14821.812319	28.853300
323.981292	14840.657159	28.858317
323.868869	14881.090243	28.863335
324.538194	14898.548350	28.868352
324.557679	14911.366797	28.873370
325.193498	14936.175155	28.878388
325.415530	14961.052039	28.883405
325.685102	14981.265249	28.888423
326.188311	15005.225645	28.893440
326.464517	15039.016082	28.898458
327.083755	15059.106890	28.903476
327.199384	15074.713473	28.908493
327.553438	15101.341857	28.913511
327.998461	15121.201517	28.918528
328.263142	15148.194671	28.923546
328.799538	15161.793051	28.928564
328.854093	15190.758120	28.933581
329.128472	15211.519313	28.938599
329.730079	15225.932849	28.943616
329.916000	15249.659262	28.948634
330.242848	15285.750870	28.953652
330.592092	15300.839852	28.958669
330.909191	15324.725918	28.963687
331.572546	15340.577815	28.968704
331.281996	15360.189119	28.973722
331.856851	15383.220889	28.978740
332.301144	15412.824805	28.983757
332.529118	15432.386622	28.988775
333.058791	15448.530273	28.993792
332.866992	15476.721746	28.998810
333.478044	15507.816076	29.003828
333.930164	15530.996037	29.008845
334.641348	15551.984834	29.013863
334.754416	15570.683179	29.018880
334.898333	15592.128438	29.023898
335.507216	15618.059793	29.028916
335.800181	15634.305853	29.033933
335.569062	15659.646537	29.038951
336.376513	15675.594699	29.043968
336.576421	15702.886348	29.048986
336.998854	15721.571489	29.054004
337.676164	15747.606784	29.059021
337.698414	15777.471930	29.064039
338.249431	15787.802544	29.069056
338.701102	15817.431187	29.074074
338.738182	15827.859500	29.079092
339.141981	15855.787539	29.084109
339.336583	15885.537662	29.089127
339.818717	15898.868226	29.094144
339.953899	15931.321997	29.099162
340.287308	15951.119172	29.104180
340.819669	15967.538726	29.109197
340.727249	16007.027110	29.114215
341.316069	16025.395033	29.119232
341.452178	16052.932677	29.124250
341.838777	16078.354603	29.129268
342.440814	16100.490740	29.134285
342.679917	16126.840328	29.139303
343.215084	16149.558192	29.144320
343.734647	16168.620244	29.149338
343.695988	16189.554276	29.154356
344.092110	16205.664033	29.159373
344.592249	16232.768158	29.164391
345.184179	16241.973162	29.169408
345.733478	16264.367294	29.174426
345.322539	16277.160317	29.179444
345.650945	16297.370135	29.184461
346.174578	16321.612794	29.189479
346.040122	16333.786347	29.194496
346.611316	16364.838454	29.199514
346.960612	16393.953882	29.204532
347.312078	16411.798802	29.209549
347.611373	16436.367215	29.214567
347.892391	16465.479883	29.219584
348.264856	16486.157093	29.224602
348.547739	16519.949461	29.229620
348.627829	16542.169428	29.234637
349.097680	16580.539970	29.239655
349.899235	16597.060614	29.244672
349.983709	16643.135263	29.249690
350.491271	16659.977326	29.254708
350.535737	16690.352731	29.259725
351.138711	16717.344479	29.264743
351.651151	16742.607887	29.269760
351.744088	16781.767946	29.274778
352.098545	16809.147759	29.279796
352.856450	16835.628561	29.284813
352.801439	16865.528949	29.289831
353.176557	16881.724811	29.294848
353.676382	16926.751046	29.299866
354.014485	16942.831718	29.304884
354.640952	16960.912298	29.309901
354.894994	16991.798969	29.314919
355.599405	17009.299231	29.319936
355.846134	17037.698208	29.324954
356.024598	17052.973118	29.329972
356.568367	17082.205744	29.334989
357.016865	17110.015011	29.340007
357.064308	17126.143970	29.345024
357.614491	17154.923259	29.350042
358.031565	17173.190054	29.355060
358.369608	17202.947180	29.360077
358.611063	17227.048713	29.365095
358.976460	17244.742475	29.370112
359.112950	17270.931167	29.375130
359.252266	17297.786222	29.380148
359.889970	17321.065668	29.385165
360.115718	17360.187770	29.390183
360.708848	17383.947584	29.395200
361.248312	17410.304675	29.400218
361.323072	17440.611809	29.405236
361.972137	17461.539237	29.410253
362.047527	17476.841055	29.415271
362.801387	17508.561825	29.420288
362.764695	17536.250338	29.425306
363.327412	17547.346236	29.430324
363.806720	17581.355746	29.435341
363.950144	17604.389515	29.440359
364.526989	17617.237615	29.445376
364.582465	17648.982814	29.450394
365.011736	17680.251622	29.455412
365.709801	17701.685140	29.460429
365.553160	17732.918605	29.465447
366.216884	17749.704406	29.470464
366.477968	17784.321099	29.475482
366.703248	17814.268233	29.480500
367.346014	17837.586977	29.485517
367.146252	17864.215318	29.490535
368.100146	17889.088981	29.495552
368.359960	17910.626833	29.500570
368.425203	17939.391585	29.505588
368.641475	17956.644176	29.510605
369.303134	17992.225967	29.515623
369.632824	18011.524929	29.520640
369.985760	18030.252560	29.525658
369.968287	18057.241987	29.530676
370.373239	18092.168131	29.535693
370.543294	18121.647305	29.540711
371.204412	18152.631132	29.545728
371.770458	18179.804783	29.550746
371.686425	18220.938093	29.555764
372.543581	18239.930898	29.560781
372.477133	18275.816668	29.565799
372.953818	18301.387892	29.570816
373.171566	18341.323910	29.575834
373.476456	18375.215727	29.580852
374.385022	18396.649987	29.585869
374.342740	18447.497272	29.590887
374.962103	18468.955844	29.595904
375.465318	18502.723662	29.600922
375.605797	18529.917873	29.605940
376.105603	18565.021636	29.610957
376.509422	18592.266951	29.615975
377.398328	18620.042116	29.620992
377.632768	18650.345516	29.626010
377.881388	18678.647666	29.631028
378.480185	18702.064761	29.636045
378.622636	18739.529680	29.641063
378.842129	18763.421097	29.646080
379.449144	18794.672039	29.651098
379.531530	18821.743915	29.656116
380.066659	18855.247047	29.661133
380.257063	18890.639175	29.666151
380.838517	18920.226662	29.671168
381.253761	18951.418201	29.676186
381.343903	18979.833796	29.681204
382.081287	19015.419431	29.686221
382.233977	19054.461434	29.691239
382.806554	19085.534171	29.696256
383.564625	19115.814813	29.701274
383.572916	19154.390655	29.706292
384.018898	19169.840791	29.711309
384.388348	19210.865221	29.716327
384.647033	19238.305874	29.721344
385.266459	19263.561718	29.726362
385.534962	19293.535884	29.731380
386.185530	19322.554555	29.736397
386.384595	19356.014990	29.741415
386.660873	19376.607668	29.746432
387.241566	19410.098065	29.751450
387.341591	19449.576947	29.756468
388.088774	19469.557356	29.761485
388.365820	19511.827519	29.766503
388.525683	19537.137764	29.771520
389.367581	19566.770002	29.776538
389.607427	19608.075409	29.781556
390.267472	19621.482007	29.786573
390.197463	19659.721975	29.791591
390.695082	19697.092417	29.796608
391.331216	19719.746436	29.801626
391.158410	19752.602320	29.806644
391.693828	19767.841138	29.811661
392.060970	19818.298472	29.816679
392.195333	19847.277362	29.821696
392.922922	19869.992124	29.826714
392.998897	19910.144539	29.831732
393.814756	19931.354906	29.836749
393.937193	19964.671578	29.841767
394.046435	19996.101745	29.846784
394.521808	20026.312580	29.851802
394.502830	20066.602481	29.856820
395.197101	20089.988380	29.861837
395.739325	20131.186695	29.866855
395.900442	20164.990839	29.871872
396.824634	20188.813383	29.876890
396.936514	20243.399232	29.881908
397.495124	20262.814264	29.886925
397.959275	20296.950062	29.891943
397.998838	20328.234720	29.896960
398.901011	20356.370052	29.901978
399.025586	20384.219472	29.906996
399.747564	20418.036936	29.912013
399.793936	20446.192653	29.917031
400.208859	20480.981815	29.922048
401.100735	20502.058925	29.927066
401.108367	20542.277764	29.932084
401.609166	20571.209870	29.937101
402.213592	20601.565930	29.942119
402.524807	20643.051266	29.947136
403.056105	20665.867391	29.952154
402.936728	20693.297313	29.957172
403.982135	20720.701635	29.962189
404.465601	20752.752397	29.967207
404.502942	20781.178202	29.972224
405.430461	20814.088976	29.977242
405.275354	20844.864437	29.982260
406.076106	20870.371767	29.987277
406.114573	20895.175963	29.992295
406.382771	20930.778674	29.997312
406.685651	20959.670099	30.002330
406.849659	21005.882352	30.007348
407.436257	21033.413570	30.012365
407.816408	21076.678105	30.017383
408.020096	21120.107550	30.022400
408.928242	21153.652873	30.027418
408.745519	21201.031461	30.032436
409.383672	21235.428903	30.037453
410.257068	21272.925133	30.042471
410.594144	21306.557388	30.047488
411.390745	21331.206797	30.052506
411.382331	21372.901344	30.057524
412.032248	21400.190906	30.062541
412.184233	21436.518712	30.067559
412.489993	21459.627092	30.072576
413.393059	21490.846680	30.077594
413.621561	21524.163071	30.082612
414.011982	21551.890008	30.087629
414.808324	21586.381818	30.092647
415.091389	21614.814083	30.097664
415.488455	21645.895380	30.102682
415.588812	21680.590863	30.107700
415.754172	21712.951530	30.112717
416.367309	21744.884960	30.117735
416.474174	21782.658974	30.122752
417.237723	21821.333520	30.127770
417.922170	21867.419423	30.132788
417.866598	21896.390694	30.137805
418.576121	21922.696796	30.142823
418.966722	21960.231883	30.147840
419.507574	21991.015660	30.152858
419.941867	22021.772978	30.157876
420.142268	22046.410151	30.162893
420.618707	22092.537399	30.167911
421.079683	22119.766364	30.172928
421.596757	22146.498861	30.177946
422.087279	22181.197024	30.182964
422.182371	22207.425500	30.187981
422.879052	22238.841463	30.192999
423.337684	22262.445985	30.198016
423.746752	22294.699627	30.203034
424.007934	22332.354719	30.208052
424.050548	22344.176921	30.213069
424.462193	22389.301812	30.218087
424.688123	22425.742492	30.223104
425.351110	22461.584261	30.228122
425.188032	22500.738537	30.233140
425.938749	22542.307173	30.238157
426.670559	22584.894520	30.243175
427.116368	22613.568012	30.248192
427.681196	22657.105622	30.253210
427.663935	22689.525180	30.258228
428.006457	22721.513123	30.263245
428.427925	22765.826891	30.268263
428.924250	22810.295533	30.273280
429.911413	22858.637817	30.278298
430.347927	22886.233162	30.283316
430.645531	22935.650089	30.288333
431.265177	22969.789208	30.293351
431.254430	23007.194346	30.298368
431.989066	23038.190794	30.303386
432.125463	23081.715242	30.308404
432.588132	23116.654882	30.313421
433.099208	23156.364540	30.318439
433.696031	23200.658306	30.323456
434.272429	23228.618972	30.328474
434.683267	23267.981218	30.333492
434.984844	23306.759262	30.338509
435.605579	23342.788074	30.343527
435.947582	23381.020296	30.348544
436.207939	23415.484690	30.353562
436.663695	23454.527706	30.358580
437.155950	23498.812745	30.363597
437.489658	23537.636457	30.368615
437.893042	23581.116420	30.373632
438.305793	23614.718650	30.378650
438.989026	23653.838016	30.383668
439.410011	23695.894544	30.388685
440.087228	23729.440619	30.393703
440.134516	23768.692298	30.398720
440.748372	23801.596147	30.403738
441.343527	23843.829219	30.408756
441.606010	23883.073934	30.413773
442.225476	23925.539728	30.418791
442.666700	23965.858922	30.423808
443.329600	23990.125903	30.428826
443.665444	24028.131935	30.433844
443.928557	24065.629688	30.438861
444.396891	24105.616716	30.443879
444.721220	24139.666703	30.448896
445.402118	24180.927619	30.453914
445.393101	24227.535237	30.458932
445.916437	24265.826165	30.463949
446.632996	24314.250484	30.468967
446.837073	24349.345832	30.473984
447.646994	24380.925217	30.479002
448.035886	24426.275316	30.484020
448.524599	24461.604498	30.489037
449.040641	24492.431604	30.494055
449.377793	24521.604124	30.499072
449.736668	24559.241658	30.504090
450.294638	24596.840019	30.509108
450.708768	24633.355198	30.514125
451.041128	24670.912207	30.519143
451.258260	24701.413824	30.524160
451.717034	24735.152574	30.529178
452.204133	24771.346874	30.534196
452.677456	24819.948501	30.539213
453.045182	24852.973959	30.544231
453.293065	24899.834218	30.549248
453.981475	24929.289945	30.554266
454.442444	24963.549207	30.559284
454.337884	25004.267114	30.564301
455.275263	25049.357772	30.569319
455.475965	25092.939777	30.574336
456.349591	25129.512445	30.579354
456.971099	25170.249373	30.584372
457.024676	25216.120709	30.589389
457.740585	25251.546396	30.594407
458.106864	25304.516687	30.599424
458.416430	25332.859299	30.604442
458.681997	25377.541558	30.609460
459.294102	25423.273704	30.614477
460.046110	25457.381701	30.619495
460.395753	25508.885522	30.624512
461.104415	25547.965585	30.629530
461.278428	25593.335401	30.634548
461.731906	25631.786036	30.639565
461.822571	25664.764277	30.644583
462.358630	25723.325445	30.649600
463.109845	25762.651293	30.654618
463.535322	25815.736376	30.659636
463.849363	25858.724335	30.664653
464.606293	25899.787551	30.669671
465.028185	25954.157443	30.674688
465.609116	25989.004520	30.679706
466.195856	26030.869013	30.684724
466.835177	26079.986116	30.689741
467.331440	26112.913866	30.694759
467.601835	26158.613039	30.699776
467.662939	26189.253516	30.704794
468.390629	26233.744811	30.709812
468.800275	26283.039290	30.714829
469.463132	26319.520045	30.719847
470.033111	26371.624005	30.724864
470.612171	26407.576263	30.729882
470.926093	26452.363708	30.734900
471.475695	26491.891768	30.739917
471.712924	26532.572492	30.744935
472.172527	26578.247773	30.749952
472.603936	26628.615286	30.754970
473.297367	26668.646735	30.759988
473.587786	26711.347364	30.765005
473.974884	26745.455213	30.770023
474.688599	26795.025741	30.775040
474.994494	26837.131086	30.780058
475.448903	26872.316329	30.785076
476.203754	26916.132990	30.790093
476.903959	26957.908404	30.795111
477.239307	26999.652816	30.800128
477.585036	27040.531283	30.805146
478.219546	27083.585972	30.810164
478.506841	27127.679275	30.815181
479.165031	27159.468688	30.820199
479.732116	27200.992276	30.825216
480.102596	27251.034150	30.830234
480.767807	27282.901491	30.835252
480.974830	27336.295528	30.840269
481.497120	27361.972235	30.845287
482.149940	27411.504133	30.850304
482.620956	27441.372373	30.855322
483.018370	27473.145580	30.860340
483.301039	27520.265867	30.865357
483.732114	27541.787598	30.870375
484.093905	27588.869742	30.875392
484.804913	27614.969855	30.880410
485.392997	27659.541550	30.885428
485.441475	27696.861899	30.890445
486.175735	27733.441079	30.895463
486.316006	27775.333205	30.900480
486.682259	27816.784244	30.905498
487.382386	27861.145484	30.910516
487.460922	27908.691778	30.915533
488.168982	27948.868881	30.920551
488.661154	28000.400696	30.925568
489.212451	28045.443203	30.930586
490.027175	28093.723093	30.935604
490.223047	28144.058271	30.940621
490.537845	28184.386170	30.945639
491.127312	28235.684909	30.950656
491.614201	28287.565466	30.955674
492.163666	28332.684733	30.960692
492.577074	28380.691119	30.965709
493.169087	28422.232431	30.970727
493.680194	28479.135036	30.975744
494.459576	28534.337191	30.980762
494.896750	28576.544907	30.985780
495.467091	28620.254442	30.990797
496.169195	28659.121789	30.995815
496.692410	28705.366309	31.000832
497.049231	28749.799243	31.005850
497.722378	28793.561606	31.010868
497.714710	28837.335784	31.015885
498.292697	28883.218374	31.020903
498.908665	28934.521094	31.025920
499.326102	28980.764918	31.030938
500.209272	29023.537190	31.035956
500.152280	29076.525951	31.040973
500.352745	29111.934421	31.045991
501.539138	29173.428281	31.051008
502.080697	29220.510324	31.056026
502.781151	29255.211684	31.061044
502.847791	29308.013478	31.066061
503.620353	29349.965652	31.071079
504.180604	29395.107966	31.076096
504.861611	29438.671886	31.081114
505.381717	29479.284294	31.086132
505.980144	29528.440004	31.091149
506.618068	29569.692507	31.096167
506.881731	29612.758032	31.101184
506.966474	29654.436695	31.106202
507.646397	29697.105432	31.111220
508.022669	29745.506617	31.116237
508.628538	29788.515947	31.121255
509.153344	29826.181634	31.126272
509.542034	29879.745843	31.131290
509.942534	29926.925693	31.136308
510.694460	29991.087733	31.141325
510.989396	30028.492166	31.146343
511.572274	30092.130421	31.151360
511.870539	30142.713115	31.156378
512.606276	30190.185254	31.161396
513.229469	30239.575488	31.166413
513.754079	30285.073047	31.171431
514.277516	30328.034239	31.176448
514.351185	30384.580023	31.181466
515.154008	30421.043067	31.186484
515.774123	30469.519481	31.191501
516.255565	30514.109798	31.196519
516.760429	30558.854108	31.201536
517.035442	30605.687395	31.206554
517.726360	30637.036021	31.211572
518.103627	30693.239131	31.216589
518.754392	30728.696246	31.221607
519.083283	30774.132802	31.226624
519.436634	30837.969493	31.231642
519.806694	30876.489692	31.236660
520.248747	30938.904864	31.241677
520.794489	30987.581167	31.246695
521.246897	31043.902324	31.251712
521.946652	31103.445221	31.256730
522.474224	31137.147159	31.261748
522.820989	31199.146754	31.266765
523.350738	31252.250066	31.271783
523.731001	31309.369662	31.276800
524.178635	31370.539113	31.281818
525.300461	31420.011068	31.286836
525.572504	31480.477933	31.291853
525.775801	31535.942624	31.296871
526.790706	31603.903859	31.301888
527.120050	31663.544644	31.306906
527.759125	31704.464347	31.311924
527.837886	31764.658098	31.316941
528.686399	31823.102839	31.321959
529.201700	31879.107027	31.326976
529.913237	31938.915839	31.331994
530.781637	31999.052299	31.337012
530.977418	32052.330023	31.342029
531.557120	32108.270638	31.347047
532.141005	32167.306186	31.352064
532.745822	32219.563798	31.357082
533.381664	32267.815359	31.362100
533.974579	32330.440823	31.367117
534.725123	32373.858508	31.372135
535.053332	32426.774656	31.377152
535.318080	32485.217202	31.382170
536.134879	32533.751934	31.387188
536.702444	32587.171695	31.392205
537.218916	32645.920220	31.397223
537.947715	32697.212079	31.402240
538.435366	32763.829258	31.407258
538.845040	32805.376387	31.412276
539.397074	32862.523053	31.417293
539.794053	32909.402207	31.422311
540.462160	32956.444888	31.427328
541.077561	33017.172572	31.432346
541.627805	33062.975972	31.437364
542.003604	33129.007158	31.442381
542.199355	33175.481685	31.447399
542.915882	33245.723270	31.452416
543.893154	33301.500879	31.457434
544.179967	33351.630763	31.462452
544.934035	33414.719345	31.467469
545.283363	33464.444749	31.472487
546.121809	33510.472997	31.477504
546.576333	33567.858955	31.482522
547.247285	33612.551941	31.487540
547.578582	33668.825733	31.492557
548.289582	33724.620325	31.497575
548.704896	33771.249414	31.502592
548.866843	33836.826317	31.507610
550.076736	33884.207822	31.512628
550.476218	33947.480031	31.517645
550.927321	33996.640982	31.522663
551.246853	34046.294043	31.527680
551.430970	34120.486628	31.532698
552.313424	34164.467514	31.537716
552.409056	34220.706298	31.542733
553.214475	34266.476877	31.547751
554.046731	34324.825235	31.552768
554.333432	34369.081924	31.557786
555.343206	34422.718037	31.562804
555.816955	34474.357012	31.567821
556.210879	34529.449187	31.572839
556.985383	34577.968086	31.577856
557.164726	34635.746987	31.582874
558.034021	34679.570371	31.587892
558.357625	34737.625536	31.592909
558.987612	34791.388710	31.597927
559.641288	34844.434899	31.602944
559.720057	34905.929995	31.607962
560.354299	34962.526963	31.612980
561.065448	35021.702383	31.617997
561.238818	35093.335016	31.623015
562.007836	35139.334765	31.628032
562.303655	35206.248414	31.633050
563.043264	35279.867862	31.638068
563.450149	35339.331367	31.643085
563.975158	35414.697406	31.648103
564.891259	35469.194794	31.653120
565.054233	35542.358429	31.658138
565.993501	35597.893853	31.663156
566.274783	35659.667303	31.668173
566.942612	35722.652041	31.673191
567.944943	35796.962333	31.678208
568.049851	35863.307206	31.683226
569.077828	35912.040254	31.688244
569.652579	35983.054543	31.693261
570.194561	36053.042494	31.698279
571.236577	36105.946090	31.703296
571.408134	36172.991194	31.708314
572.005241	36226.293836	31.713332
572.779189	36286.807529	31.718349
573.063259	36345.657135	31.723367
573.941718	36407.864566	31.728384
574.486279	36467.413163	31.733402
575.226057	36519.443226	31.738420
575.249283	36587.410758	31.743437
575.725007	36653.899172	31.748455
576.286771	36719.208954	31.753472
576.860714	36787.812044	31.758490
577.332314	36851.603303	31.763508
578.111687	36911.771004	31.768525
578.469776	36993.426904	31.773543
579.279716	37053.656301	31.778560
579.996052	37122.533786	31.783578
580.395199	37186.436054	31.788596
580.950429	37256.555873	31.793613
581.628422	37344.687642	31.798631
582.225746	37389.727299	31.803648
582.829954	37462.873032	31.808666
583.477292	37527.754931	31.813684
584.176382	37595.450279	31.818701
584.264426	37668.022562	31.823719
585.329858	37720.766034	31.828736
585.591570	37806.494319	31.833754
586.011612	37864.022760	31.838772
586.447499	37941.995998	31.843789
587.252215	38020.277847	31.848807
588.078442	38070.770346	31.853824
588.293017	38155.494854	31.858842
589.073785	38221.629200	31.863860
589.882164	38287.825503	31.868877
590.406101	38363.200822	31.873895
591.031368	38425.914753	31.878912
591.508176	38492.595943	31.883930
591.854601	38550.085068	31.888948
592.885266	38610.491431	31.893965
592.856871	38682.812394	31.898983
593.766562	38735.126876	31.904000
594.327988	38801.211229	31.909018
594.993921	38865.974865	31.914036
595.521763	38931.942141	31.919053
595.879624	38994.023600	31.924071
596.980713	39064.495669	31.929088
597.668005	39129.215668	31.934106
597.533352	39194.318105	31.939124
598.496746	39264.283412	31.944141
599.088909	39339.149557	31.949159
599.672198	39404.758974	31.954176
600.298915	39474.768161	31.959194
600.771341	39544.137082	31.964212
601.367919	39609.609295	31.969229
601.712259	39686.282455	31.974247
602.341649	39756.412230	31.979264
603.184499	39839.086561	31.984282
603.744760	39911.147662	31.989300
604.451856	39977.407872	31.994317
605.077961	40065.965413	31.999335
605.856352	40136.469740	32.004352
606.993060	40207.770547	32.009370
607.093299	40278.845356	32.014388
607.655559	40338.624635	32.019405
608.364713	40423.063122	32.024423
609.129843	40487.459346	32.029440
609.733673	40561.823444	32.034458
610.265031	40625.261257	32.039476
610.922223	40694.259844	32.044493
611.188936	40776.484409	32.049511
612.166588	40843.369078	32.054528
612.745058	40920.352740	32.059546
613.266233	40983.244163	32.064564
614.050025	41056.024108	32.069581
614.703224	41133.176239	32.074599
615.181278	41190.408756	32.079616
615.559769	41269.602112	32.084634
616.541503	41343.616391	32.089652
617.279308	41410.934266	32.094669
617.507831	41481.957748	32.099687
618.151069	41554.235686	32.104704
618.772625	41643.694986	32.109722
619.581543	41710.591768	32.114740
619.842860	41787.426300	32.119757
620.906619	41864.021046	32.124775
621.613306	41944.457391	32.129792
622.148195	42015.242801	32.134810
622.569902	42082.081859	32.139828
623.469669	42150.815273	32.144845
623.914583	42209.843359	32.149863
624.575257	42288.530277	32.154880
625.016336	42362.170814	32.159898
625.795315	42441.694400	32.164916
626.168463	42508.555654	32.169933
627.015569	42601.774043	32.174951
627.656005	42665.083975	32.179968
628.498984	42745.535967	32.184986
629.107883	42817.136222	32.190004
629.603291	42882.690433	32.195021
630.125005	42963.247032	32.200039
630.883622	43038.956239	32.205056
631.897232	43108.002713	32.210074
631.720563	43189.714583	32.215092
632.981980	43248.279356	32.220109
633.253730	43321.181308	32.225127
634.150444	43373.842613	32.230144
634.427283	43443.514240	32.235162
635.099065	43512.637709	32.240180
635.653018	43575.245160	32.245197
635.867443	43651.681515	32.250215
636.901422	43725.582968	32.255232
637.673639	43793.532093	32.260250
637.765341	43867.507906	32.265268
638.798764	43948.988155	32.270285
639.461154	44029.652371	32.275303
639.782462	44091.302281	32.280320
640.210192	44178.200900	32.285338
640.960889	44257.029620	32.290356
641.549893	44331.019709	32.295373
642.528963	44423.237051	32.300391
643.028104	44489.920351	32.305408
643.516722	44581.828078	32.310426
644.101961	44663.297167	32.315444
645.051082	44734.377992	32.320461
645.661554	44825.130023	32.325479
646.468409	44894.567785	32.330496
647.091322	44979.593780	32.335514
647.614107	45062.461120	32.340532
648.544722	45144.178282	32.345549
649.001737	45233.132551	32.350567
649.718093	45307.275924	32.355584
650.602028	45378.164717	32.360602
650.903091	45462.529343	32.365620
652.056906	45537.842222	32.370637
652.348927	45630.472809	32.375655
653.019252	45707.363112	32.380672
653.553614	45791.914810	32.385690
654.305452	45870.715361	32.390708
655.464314	45953.617163	32.395725
655.929442	46030.151163	32.400743
656.415624	46100.382179	32.405760
657.204693	46190.776500	32.410778
657.960479	46262.823469	32.415796
658.661793	46343.825879	32.420813
659.173625	46427.354686	32.425831
660.037333	46504.017287	32.430848
660.633400	46580.857108	32.435866
661.263809	46667.572602	32.440884
662.057574	46739.214045	32.445901
662.300073	46822.448093	32.450919
663.105385	46898.196678	32.455936
663.988870	46979.642195	32.460954
664.214797	47065.595881	32.465972
665.484270	47142.105509	32.470989
665.635730	47230.674428	32.476007
666.358120	47315.151277	32.481024
667.076779	47395.848976	32.486042
667.485873	47479.914158	32.491060
668.531817	47555.685554	32.496077
669.100678	47644.683155	32.501095
669.531736	47726.513045	32.506112
670.582116	47810.940988	32.511130
670.829297	47900.384599	32.516148
672.133536	47977.412919	32.521165
672.300130	48066.100058	32.526183
673.019626	48141.413012	32.531200
673.840876	48234.372964	32.536218
673.967839	48314.960838	32.541236
675.126678	48396.682671	32.546253
675.582220	48496.955578	32.551271
676.217656	48573.111584	32.556288
676.945615	48669.386251	32.561306
677.618147	48742.299613	32.566324
678.514868	48819.496648	32.571341
678.730462	48902.267308	32.576359
679.432437	48978.256002	32.581376
680.322693	49065.264697	32.586394
680.852584	49154.664230	32.591412
681.616288	49219.851749	32.596429
681.959389	49316.297551	32.601447
682.694683	49397.342035	32.606464
683.807138	49479.205647	32.611482
684.291204	49564.941499	32.616500
684.722418	49647.085918	32.621517
685.095520	49751.683884	32.626535
686.533027	49836.558892	32.631552
687.243552	49922.047255	32.636570
687.651601	50006.824851	32.641588
688.470609	50089.864010	32.646605
689.451435	50177.958735	32.651623
689.929163	50264.207256	32.656640
690.727465	50342.639541	32.661658
691.161129	50438.858033	32.666676
691.962345	50522.805332	32.671693
692.327729	50610.969099	32.676711
692.936963	50707.254637	32.681728
693.837670	50804.307347	32.686746
694.452280	50902.696576	32.691764
695.709207	50989.312164	32.696781
696.281719	51081.417328	32.701799
696.738372	51182.512615	32.706816
697.636796	51264.179145	32.711834
698.094555	51364.883525	32.716852
699.279089	51450.508694	32.721869
699.775089	51531.680676	32.726887
700.262331	51633.006988	32.731904
701.300486	51719.156632	32.736922
701.696085	51820.619111	32.741940
702.376174	51900.170172	32.746957
703.018303	51999.640692	32.751975
703.910191	52095.267229	32.756992
704.798529	52181.879616	32.762010
705.543444	52278.276840	32.767028
706.182556	52369.859037	32.772045
707.170253	52465.958001	32.777063
707.821170	52551.663652	32.782080
708.450868	52636.722462	32.787098
708.618058	52740.906228	32.792116
709.550723	52829.523206	32.797133
710.411642	52916.446640	32.802151
710.958908	53019.690836	32.807168
711.943529	53105.135219	32.812186
712.338963	53214.255922	32.817204
712.935777	53304.042560	32.822221
713.968178	53405.603774	32.827239
714.587125	53495.949929	32.832256
715.811294	53580.920815	32.837274
716.330181	53671.827683	32.842292
717.108331	53771.082524	32.847309
717.506974	53860.000995	32.852327
718.342191	53950.250281	32.857344
719.117764	54044.945217	32.862362
719.784590	54142.312251	32.867380
720.470341	54221.890758	32.872397
721.276201	54332.643061	32.877415
721.931134	54425.161018	32.882432
723.035586	54500.539211	32.887450
723.369050	54599.423183	32.892468
724.154722	54688.938479	32.897485
724.785164	54776.495873	32.902503
725.665127	54878.064625	32.907520
726.471059	54958.024282	32.912538
726.977195	55045.584475	32.917556
727.880044	55118.256143	32.922573
728.483783	55198.768340	32.927591
728.854060	55288.784728	32.932608
729.985578	55373.159447	32.937626
730.701631	55466.588364	32.942644
731.312417	55549.723059	32.947661
732.275522	55637.880056	32.952679
732.941940	55731.154143	32.957696
733.525933	55797.764519	32.962714
734.207707	55897.387192	32.967732
735.099213	55982.189651	32.972749
735.486348	56072.617524	32.977767
736.308039	56167.188609	32.982784
737.349190	56263.733251	32.987802
737.978159	56360.649851	32.992820
738.412515	56455.242144	32.997837
739.324253	56545.755998	33.002855
739.842286	56630.882078	33.007872
741.007878	56728.729062	33.012890
741.816373	56835.336967	33.017908
742.389264	56925.384111	33.022925
743.393158	57017.464637	33.027943
743.919620	57121.049619	33.032960
744.863322	57203.036608	33.037978
745.573647	57301.732650	33.042996
746.287978	57390.361942	33.048013
747.540975	57480.848860	33.053031
748.011889	57578.353608	33.058048
748.724197	57660.943168	33.063066
749.164376	57770.290059	33.068084
750.088486	57852.561001	33.073101
751.147668	57944.655605	33.078119
751.654899	58043.812296	33.083136
752.533779	58135.735378	33.088154
753.134359	58231.907396	33.093172
753.779003	58328.704539	33.098189
754.687982	58424.339857	33.103207
755.147016	58525.314292	33.108224
756.209457	58615.566104	33.113242
756.817132	58717.818762	33.118260
757.622574	58817.498704	33.123277
758.082192	58924.485078	33.128295
758.817918	59022.085730	33.133312
759.623642	59121.994640	33.138330
760.486781	59233.036409	33.143348
761.135661	59330.507559	33.148365
762.189033	59427.040126	33.153383
763.076781	59536.354158	33.158400
763.781958	59626.814945	33.163418
764.291984	59737.810453	33.168436
765.343679	59838.838773	33.173453
766.057814	59927.428694	33.178471
766.660469	60036.388097	33.183488
767.753549	60122.919044	33.188506
768.470538	60226.090294	33.193524
769.439647	60320.233079	33.198541
770.416011	60413.477633	33.203559
770.871158	60518.178923	33.208576
771.707157	60607.371033	33.213594
772.208061	60709.980055	33.218612
772.944392	60800.207063	33.223629
773.925567	60899.962979	33.228647
774.256525	61006.836239	33.233664
775.251421	61103.904720	33.238682
776.018905	61211.623307	33.243700
776.738928	61299.693628	33.248717
777.661654	61397.761439	33.253735
777.936920	61480.818102	33.258752
778.894261	61572.712190	33.263770
779.595797	61670.084707	33.268788
780.594535	61768.748500	33.273805
781.297729	61858.498975	33.278823
781.891177	61960.214073	33.283840
782.572247	62057.560213	33.288858
783.193869	62152.135525	33.293876
783.711476	62262.315490	33.298893
784.997553	62363.816889	33.303911
785.701710	62474.871012	33.308928
786.729307	62572.295012	33.313946
787.187991	62682.442728	33.318964
788.007582	62787.348172	33.323981
788.877924	62877.960384	33.328999
789.969839	62983.624546	33.334016
790.701650	63087.876015	33.339034
791.264103	63202.832288	33.344052
792.181376	63309.456202	33.349069
792.837831	63407.508118	33.354087
793.513577	63526.606751	33.359104
794.446389	63623.476172	33.364122
795.331886	63739.532453	33.369140
796.179688	63841.145229	33.374157
796.909090	63950.534305	33.379175
797.509495	64078.308737	33.384192
798.442809	64182.140469	33.389210
799.355399	64291.444151	33.394228
800.232890	64398.541716	33.399245
801.213541	64503.201653	33.404263
802.016937	64624.757169	33.409280
802.960922	64734.557387	33.414298
803.515204	64838.752206	33.419316
804.517068	64950.851361	33.424333
805.534288	65046.897981	33.429351
806.429459	65150.797755	33.434368
806.795270	65252.219001	33.439386
808.227481	65365.557795	33.444404
808.633312	65475.198059	33.449421
809.901677	65578.873873	33.454439
810.115612	65680.183237	33.459456
811.134330	65781.543313	33.464474
812.124277	65891.759262	33.469492
812.439177	66006.455884	33.474509
813.687100	66107.849171	33.479527
814.559936	66225.969710	33.484544
815.152620	66318.160123	33.489562
815.885961	66426.847151	33.494580
816.916219	66536.560383	33.499597
817.853105	66648.451790	33.504615
818.188559	66755.885010	33.509632
819.228884	66866.540298	33.514650
820.043711	66974.767806	33.519668
820.913507	67094.828325	33.524685
821.850231	67193.553444	33.529703
822.317953	67310.678617	33.534720
823.389608	67409.293917	33.539738
824.016562	67527.437141	33.544756
825.020957	67641.352136	33.549773
825.986063	67743.868576	33.554791
826.666565	67859.678146	33.559808
827.255747	67964.616112	33.564826
828.016616	68075.241767	33.569844
828.904585	68187.054588	33.574861
829.986168	68296.319582	33.579879
830.652678	68416.383294	33.584896
830.930533	68518.100368	33.589914
832.272086	68628.544350	33.594932
833.180101	68732.921245	33.599949
833.814304	68824.451843	33.604967
834.602114	68939.307468	33.609984
835.158916	69044.192897	33.615002
836.359170	69144.268220	33.620020
837.032386	69258.379454	33.625037
837.625152	69370.601407	33.630055
838.538007	69472.660619	33.635072
839.374320	69581.163445	33.640090
840.032295	69704.776699	33.645108
840.758219	69824.889107	33.650125
841.613330	69947.206547	33.655143
842.133762	70071.527562	33.660160
843.136131	70198.785735	33.665178
844.199050	70319.509112	33.670196
844.917560	70444.962999	33.675213
845.975794	70565.277525	33.680231
846.785894	70691.780015	33.685248
847.721681	70800.816372	33.690266
848.726764	70920.016122	33.695284
849.447349	71052.447892	33.700301
850.571112	71159.045756	33.705319
851.231583	71289.844833	33.710336
851.898692	71414.275824	33.715354
852.989189	71529.664389	33.720372
853.679395	71653.865293	33.725389
854.954500	71785.052633	33.730407
856.148463	71903.543632	33.735424
856.454319	72026.659340	33.740442
857.142773	72146.013087	33.745460
858.299520	72280.720031	33.750477
859.232885	72388.089010	33.755495
859.884562	72510.973206	33.760512
860.707922	72641.525856	33.765530
862.066915	72765.982989	33.770548
862.731651	72886.236402	33.775565
864.117260	73009.634430	33.780583
864.739504	73134.221844	33.785600
865.626821	73248.957527	33.790618
866.433469	73362.916646	33.795636
867.001446	73495.584632	33.800653
868.168172	73611.762183	33.805671
869.014516	73742.640165	33.810688
869.871609	73864.125673	33.815706
870.772516	73977.376745	33.820724
871.632185	74113.073828	33.825741
872.435454	74227.398500	33.830759
873.443475	74365.943863	33.835776
874.463427	74485.780522	33.840794
875.275909	74609.554330	33.845812
875.497970	74721.789444	33.850829
876.976114	74853.164072	33.855847
877.669933	74988.723238	33.860864
878.497486	75103.946545	33.865882
879.333894	75228.504128	33.870900
880.408287	75357.861420	33.875917
881.167190	75481.332761	33.880935
881.921069	75609.378402	33.885952
882.812217	75733.683121	33.890970
883.686632	75859.800201	33.895988
884.409405	75988.542587	33.901005
885.732952	76114.485643	33.906023
886.122728	76239.508611	33.911040
886.970811	76363.583645	33.916058
888.140184	76492.324674	33.921076
888.728011	76629.973380	33.926093
890.088285	76736.850295	33.931111
891.145150	76860.362275	33.936128
891.842039	76975.515739	33.941146
892.822094	77080.382549	33.946164
893.384839	77203.839001	33.951181
894.361338	77314.109209	33.956199
895.211949	77441.314498	33.961216
895.854610	77563.848890	33.966234
897.074219	77677.293934	33.971252
897.691211	77801.567013	33.976269
898.443479	77922.731621	33.981287
899.274838	78050.145974	33.986304
899.972442	78175.008710	33.991322
901.174874	78309.884145	33.996340
901.816382	78447.503556	34.001357
902.934313	78567.852117	34.006375
903.712276	78712.446667	34.011392
904.556037	78846.106869	34.016410
905.511735	78979.192693	34.021428
906.314683	79128.568004	34.026445
907.443875	79254.813960	34.031463
908.149497	79396.907216	34.036480
908.725903	79531.640481	34.041498
910.169861	79672.525326	34.046516
911.023988	79813.767956	34.051533
911.906859	79947.674932	34.056551
913.207809	80082.266353	34.061568
914.060945	80234.810004	34.066586
914.864154	80359.749620	34.071604
915.648496	80511.920621	34.076621
916.628048	80643.740756	34.081639
918.056663	80781.870516	34.086656
918.821626	80921.932820	34.091674
919.832595	81052.326728	34.096692
920.589555	81183.699682	34.101709
921.466065	81327.813847	34.106727
922.235038	81469.359217	34.111744
923.154782	81612.069898	34.116762
924.407284	81748.273455	34.121780
924.980413	81902.974973	34.126797
926.272592	82031.638797	34.131815
927.089203	82181.158457	34.136832
927.875465	82324.433414	34.141850
929.275325	82453.897937	34.146868
929.799982	82597.470927	34.151885
930.826165	82741.139023	34.156903
931.455839	82888.720265	34.161920
932.509123	83033.005726	34.166938
933.635615	83167.327853	34.171956
934.685135	83313.172096	34.176973
935.334058	83462.221664	34.181991
936.606050	83598.211529	34.187008
937.563158	83748.224293	34.192026
938.264064	83871.409444	34.197044
939.243224	84025.842962	34.202061
940.159880	84172.435886	34.207079
941.147573	84306.268762	34.212096
941.907542	84461.456397	34.217114
942.751545	84601.496413	34.222132
943.511925	84742.614083	34.227149
944.847259	84895.229174	34.232167
946.032091	85039.049817	34.237184
947.000982	85187.488093	34.242202
948.232119	85323.032925	34.247220
948.671702	85474.787550	34.252237
949.779546	85610.949225	34.257255
950.797804	85755.137186	34.262272
951.148828	85890.128490	34.267290
952.285637	86031.147408	34.272308
953.427237	86163.959404	34.277325
954.514122	86305.007209	34.282343
955.554481	86441.880921	34.287360
956.160605	86579.320805	34.292378
957.383429	86704.016550	34.297396
958.047589	86842.638002	34.302413
959.380910	86974.941963	34.307431
960.295273	87101.000691	34.312448
960.542523	87246.945252	34.317466
961.830506	87387.396773	34.322484
962.801257	87527.085274	34.327501
963.206690	87672.481076	34.332519
964.370323	87818.353562	34.337536
965.211718	87976.487226	34.342554
966.341123	88129.688956	34.347572
967.175979	88281.560829	34.352589
968.277397	88439.205273	34.357607
969.275058	88586.748951	34.362624
969.933505	88752.062691	34.367642
970.828963	88903.820933	34.372660
971.963050	89055.603964	34.377677
972.977831	89222.444149	34.382695
974.111472	89377.172041	34.387712
974.855479	89534.053790	34.392730
976.285643	89697.278278	34.397748
977.332597	89857.890230	34.402765
977.970387	90012.248558	34.407783
979.124176	90162.472167	34.412800
980.276271	90318.804256	34.417818
981.714182	90476.298902	34.422836
982.280747	90635.381641	34.427853
983.121136	90790.951919	34.432871
984.481946	90945.494132	34.437888
984.859536	91108.655428	34.442906
985.914547	91266.851451	34.447924
987.302383	91440.113596	34.452941
988.071440	91595.852747	34.457959
989.511674	91745.133786	34.462976
990.099775	91909.063134	34.467994
991.117268	92063.409760	34.473012
991.866514	92229.561497	34.478029
992.970678	92391.503654	34.483047
994.342837	92551.029066	34.488064
994.932188	92731.128908	34.493082
996.296538	92885.442378	34.498100
997.125132	93051.073907	34.503117
998.220140	93215.567498	34.508135
999.241601	93372.244686	34.513152
999.993554	93541.974778	34.518170
1001.097359	93704.153558	34.523188
1002.355092	93870.529862	34.528205
1003.010278	94035.253589	34.533223
1004.668309	94197.331323	34.538240
1005.170948	94365.247369	34.543258
1006.062312	94524.662578	34.548276
1007.167899	94699.520004	34.553293
1008.352068	94865.459438	34.558311
1009.368281	95019.375463	34.563328
1010.218508	95196.671363	34.568346
1011.300712	95356.668063	34.573364
1012.673654	95517.668520	34.578381
1013.436369	95681.701784	34.583399
1014.695464	95842.166117	34.588416
1015.397445	96008.541091	34.593434
1016.523990	96173.555597	34.598452
1017.589395	96330.617763	34.603469
1018.645982	96498.488300	34.608487
1019.823473	96633.162350	34.613504
1020.529439	96796.826180	34.618522
1021.472978	96938.415413	34.623540
1022.447127	97098.966594	34.628557
1023.559898	97245.973824	34.633575
1024.704792	97391.216702	34.638592
1025.591243	97546.075056	34.643610
1026.447770	97705.155535	34.648628
1027.414351	97865.681214	34.653645
1028.257823	98028.526333	34.658663
1029.835856	98184.610051	34.663680
1030.594724	98346.356991	34.668698
1031.421364	98499.540761	34.673716
1032.716562	98667.183741	34.678733
1033.412774	98830.172330	34.683751
1034.317017	98992.785695	34.688768
1035.431531	99157.891416	34.693786
1036.764253	99340.163652	34.698804
1037.893045	99500.337330	34.703821
1038.696054	99673.835984	34.708839
1039.726772	99835.116942	34.713856
1040.600840	100010.239584	34.718874
1041.851934	100175.240679	34.723892
1042.762977	100351.923375	34.728909
1043.572943	100534.968034	34.733927
1044.934325	100703.031342	34.738944
1046.193682	100898.299895	34.743962
1047.331520	101055.221116	34.748980
1048.475092	101232.650203	34.753997
1049.323934	101402.221096	34.759015
1050.530849	101564.357558	34.764032
1051.615131	101747.232524	34.769050
1052.170443	101923.168046	34.774068
1053.506009	102097.513120	34.779085
1054.498667	102280.698268	34.784103
1055.331217	102456.648560	34.789120
1056.611401	102648.640683	34.794138
1057.766281	102828.852219	34.799156
1058.662586	103003.086048	34.804173
1059.367238	103189.003643	34.809191
1060.834366	103366.729446	34.814208
1062.001045	103556.055900	34.819226
1063.233870	103737.305625	34.824244
1064.469348	103918.720805	34.829261
1065.107889	104109.113740	34.834279
1066.510808	104281.094034	34.839296
1067.338617	104472.433481	34.844314
1068.835706	104643.691358	34.849332
1070.086015	104821.551532	34.854349
1071.065349	105000.724201	34.859367
1071.940662	105174.735300	34.864384
1072.933599	105353.844790	34.869402
1074.181498	105545.591174	34.874420
1075.239563	105717.219904	34.879437
1076.449468	105894.714024	34.884455
1077.627370	106075.165666	34.889472
1078.591666	106250.017698	34.894490
1079.470220	106429.533328	34.899508
1080.787827	106605.481849	34.904525
1081.938419	106789.273920	34.909543
1083.032825	106969.517443	34.914560
1083.883521	107142.608224	34.919578
1084.816142	107315.876569	34.924596
1086.151497	107506.064688	34.929613
1087.149850	107691.952704	34.934631
1088.267884	107860.596085	34.939648
1089.286686	108047.281152	34.944666
1090.136734	108222.291619	34.949684
1091.467959	108392.106394	34.954701
1091.911637	108569.744939	34.959719
1093.029425	108740.661188	34.964736
1094.408213	108912.232038	34.969754
1094.977909	109098.162613	34.974772
1096.346940	109271.232038	34.979789
1097.581274	109455.446475	34.984807
1098.664419	109626.386702	34.989824
1099.467537	109810.915515	34.994842
1100.746701	109992.529403	34.999860
1102.055926	110183.792054	35.004877
1102.728011	110368.143619	35.009895
1104.089458	110551.128370	35.014912
1104.819234	110748.419170	35.019930
1106.222067	110933.451785	35.024948
1107.459551	111118.474981	35.029965
1108.184734	111314.972538	35.034983
1109.813184	111493.308319	35.040000
1110.695854	111693.190218	35.045018
1111.878414	111882.484091	35.050036
1113.078392	112063.288673	35.055053
1114.051643	112262.070242	35.060071
1115.146666	112463.404789	35.065088
1116.232130	112655.975781	35.070106
1117.432090	112848.972579	35.075124
1118.699369	113032.230052	35.080141
1119.584887	113248.414587	35.085159
1120.608831	113442.648129	35.090176
1121.968882	113644.200774	35.095194
1122.922389	113839.221520	35.100212
1124.450431	114044.321939	35.105229
1125.203183	114246.270706	35.110247
1126.769477	114438.128357	35.115264
1128.057032	114636.266736	35.120282
1128.870551	114831.203485	35.125300
1130.242119	115028.177807	35.130317
1131.589572	115232.911317	35.135335
1132.509810	115412.339449	35.140352
1133.844390	115622.171136	35.145370
1134.954782	115818.015838	35.150388
1136.198403	116011.115816	35.155405
1137.101037	116210.203077	35.160423
1138.406430	116401.749740	35.165440
1139.567168	116601.025123	35.170458
1140.633690	116813.190550	35.175476
1142.172362	116992.754469	35.180493
1143.003180	117196.181090	35.185511
1144.020848	117399.375532	35.190528
1145.498023	117599.327770	35.195546
1146.177764	117797.195841	35.200564
1147.784150	117986.004453	35.205581
1148.831462	118196.320649	35.210599
1149.990605	118392.846452	35.215616
1151.283363	118587.666240	35.220634
1152.270598	118788.683388	35.225652
1153.445727	118978.038606	35.230669
1154.592321	119195.479584	35.235687
1155.684768	119386.105595	35.240704
1156.879958	119581.771823	35.245722
1157.875797	119790.511453	35.250740
1159.228982	119988.713962	35.255757
1160.101467	120191.102955	35.260775
1161.454037	120393.477338	35.265792
1162.784175	120594.475576	35.270810
1163.692584	120794.379073	35.275828
1165.248557	120989.893680	35.280845
1166.131668	121201.513213	35.285863
1167.502229	121389.229657	35.290880
1168.676878	121568.666570	35.295898
1169.412215	121759.823224	35.300916
1170.559920	121944.323194	35.305933
1171.984494	122137.079136	35.310951
1172.974513	122319.655915	35.315968
1174.392604	122505.179178	35.320986
1175.289972	122702.588151	35.326004
1176.771355	122891.423655	35.331021
1177.314578	123090.642606	35.336039
1178.582785	123281.302713	35.341056
1179.610781	123479.747087	35.346074
1180.261993	123685.073303	35.351092
1182.128861	123896.384583	35.356109
1182.791752	124108.669458	35.361127
1183.790915	124306.072142	35.366144
1185.334486	124530.887983	35.371162
1185.986480	124737.881479	35.376180
1187.683994	124958.023770	35.381197
1188.893735	125174.332042	35.386215
1189.810852	125389.625606	35.391232
1191.286305	125604.600258	35.396250
1192.163333	125836.202525	35.401268
1192.995697	126057.725176	35.406285
1194.510679	126272.964153	35.411303
1195.586546	126511.801087	35.416320
1196.887336	126734.227122	35.421338
1198.283789	126967.894068	35.426356
1199.546016	127188.276455	35.431373
1200.593477	127414.678454	35.436391
1201.773317	127639.463180	35.441408
1203.113030	127865.515962	35.446426
1204.499034	128101.462027	35.451444
1206.131964	128327.089441	35.456461
1206.975080	128551.632218	35.461479
1208.582238	128782.882361	35.466496
1209.439361	129011.025942	35.471514
1210.946387	129233.118891	35.476532
1212.353867	129452.289106	35.481549
1213.652968	129690.745960	35.486567
1214.869871	129902.636884	35.491584
1216.436080	130123.027764	35.496602
1217.497820	130338.420475	35.501620
1218.968997	130566.879449	35.506637
1220.058453	130780.115635	35.511655
1221.231757	130988.078723	35.516672
1222.936723	131214.640293	35.521690
1223.764520	131442.083706	35.526708
1224.999246	131655.352442	35.531725
1226.127533	131869.058524	35.536743
1227.342494	132092.398706	35.541760
1228.562639	132305.331905	35.546778
1229.441276	132529.402589	35.551796
1231.033917	132757.819113	35.556813
1232.314638	132980.634829	35.561831
1233.357740	133213.531689	35.566848
1234.514597	133431.490266	35.571866
1235.664951	133659.555236	35.576884
1237.159566	133883.444729	35.581901
1237.800921	134110.798317	35.586919
1239.015217	134348.784055	35.591936
1240.409142	134575.179752	35.596954
1241.629053	134807.500958	35.601972
1243.169301	135043.257279	35.606989
1244.421207	135269.681243	35.612007
1245.356260	135503.791337	35.617024
1246.497052	135738.211392	35.622042
1247.416192	135965.950274	35.627060
1249.114606	136198.164147	35.632077
1250.318090	136419.684792	35.637095
1251.537833	136647.010983	35.642112
1252.769573	136854.329922	35.647130
1253.981483	137084.563787	35.652148
1255.226725	137299.553857	35.657165
1256.454341	137521.597655	35.662183
1257.311574	137749.067329	35.667200
1258.687968	137971.064148	35.672218
1259.691046	138207.743135	35.677236
1261.028597	138437.166716	35.682253
1262.520317	138677.800208	35.687271
1263.482005	138911.562047	35.692288
1264.407721	139139.625688	35.697306
1266.003874	139390.276411	35.702324
1267.302139	139630.580917	35.707341
1268.820049	139875.948055	35.712359
1270.001110	140124.390426	35.717376
1271.336798	140361.359085	35.722394
1272.494085	140605.307499	35.727412
1274.178541	140842.171102	35.732429
1275.304420	141087.738490	35.737447
1276.314413	141341.581623	35.742464
1277.772338	141580.427804	35.747482
1278.768970	141827.163022	35.752500
1280.498049	142072.320664	35.757517
1281.972084	142317.331975	35.762535
1282.981616	142569.218638	35.767552
1284.503338	142813.477379	35.772570
1285.572475	143073.841264	35.777588
1286.855139	143314.769886	35.782605
1288.116096	143560.902977	35.787623
1289.198179	143827.712266	35.792640
1290.778208	144077.993679	35.797658
1291.986570	144330.557521	35.802676
1293.364803	144582.549778	35.807693
1294.896986	144830.155929	35.812711
1296.163125	145086.291761	35.817728
1297.357940	145342.187579	35.822746
1298.751598	145598.749853	35.827764
1300.249887	145855.157163	35.832781
1301.590477	146110.501711	35.837799
1303.077715	146366.914482	35.842816
1304.435502	146612.063355	35.847834
1305.706330	146866.283368	35.852852
1306.558909	147120.789883	35.857869
1308.456535	147365.879974	35.862887
1309.615343	147623.167552	35.867904
1311.152758	147878.124178	35.872922
1312.388296	148128.807678	35.877940
1314.041921	148373.488256	35.882957
1315.503060	148622.336876	35.887975
1316.426030	148870.832216	35.892992
1318.030956	149110.744261	35.898010
1319.312053	149349.671366	35.903028
1320.433290	149604.429653	35.908045
1322.135633	149857.191146	35.913063
1323.180536	150089.503315	35.918080
1324.688003	150341.704172	35.923098
1326.141778	150592.558461	35.928116
1327.387847	150840.734462	35.933133
1328.708179	151073.590631	35.938151
1330.072749	151333.406574	35.943168
1331.538325	151568.068239	35.948186
1332.595609	151815.140280	35.953204
1333.844647	152057.539889	35.958221
1335.396856	152310.710448	35.963239
1336.447950	152550.659819	35.968256
1337.849319	152797.884289	35.973274
1339.161823	153032.466085	35.978292
1340.412970	153269.025531	35.983309
1341.529581	153486.632696	35.988327
1342.573458	153724.573738	35.993344
1344.179872	153963.793207	35.998362
1345.437860	154202.906832	36.003380
1347.112693	154444.375825	36.008397
1348.359425	154679.295569	36.013415
1349.664679	154929.023053	36.018432
1351.284823	155166.192660	36.023450
1352.456763	155404.921928	36.028468
1353.293992	155648.033599	36.033485
1354.688031	155891.993450	36.038503
1355.929863	156151.709761	36.043520
1357.385363	156392.313605	36.048538
1358.424467	156654.375446	36.053556
1359.577044	156916.509053	36.058573
1361.331369	157171.694675	36.063591
1362.733951	157434.881321	36.068608
1364.118481	157695.636995	36.073626
1365.629537	157966.344563	36.078644
1367.000856	158222.094890	36.083661
1368.293141	158473.736922	36.088679
1369.455783	158743.720725	36.093696
1370.818689	159007.051009	36.098714
1372.359022	159271.749161	36.103732
1373.899821	159540.825752	36.108749
1375.469163	159803.074065	36.113767
1376.669624	160070.637244	36.118784
1378.129877	160337.296530	36.123802
1379.335315	160610.571365	36.128820
1380.867954	160876.016913	36.133837
1382.035873	161145.152876	36.138855
1383.189932	161422.691633	36.143872
1385.368432	161701.788368	36.148890
1386.524673	161963.649153	36.153908
1387.823752	162248.692869	36.158925
1389.323218	162511.388437	36.163943
1390.594238	162793.268636	36.168960
1392.075760	163056.198916	36.173978
1393.430098	163338.145080	36.178996
1394.848916	163611.518303	36.184013
1396.362914	163885.613427	36.189031
1397.681638	164169.956235	36.194048
1399.289470	164446.272473	36.199066
1400.751631	164708.302549	36.204084
1401.502291	164991.754978	36.209101
1403.448326	165270.850009	36.214119
1404.922598	165558.386306	36.219136
1406.240245	165830.381867	36.224154
1407.535346	166118.395537	36.229172
1408.807817	166396.238706	36.234189
1410.639804	166670.895164	36.239207
1411.831967	166951.813026	36.244224
1413.478413	167234.472071	36.249242
1414.945563	167516.604234	36.254260
1416.271159	167795.982716	36.259277
1417.902511	168076.555924	36.264295
1419.139177	168355.914518	36.269312
1420.485585	168625.879486	36.274330
1422.061395	168907.786705	36.279348
1422.992379	169191.363007	36.284365
1425.061613	169461.911406	36.289383
1426.237075	169746.783137	36.294400
1427.581302	170026.946340	36.299418
1429.012499	170308.924170	36.304436
1430.445209	170582.363369	36.309453
1432.068472	170862.016019	36.314471
1432.866898	171135.296812	36.319488
1434.711647	171392.721675	36.324506
1436.190704	171656.984794	36.329524
1436.944071	171922.866739	36.334541
1439.057883	172180.099190	36.339559
1440.196700	172458.788169	36.344576
1441.541721	172717.495743	36.349594
1443.020530	172994.456587	36.354612
1444.713439	173265.127332	36.359629
1446.177103	173535.748661	36.364647
1447.426698	173812.092226	36.369664
1448.833699	174083.652415	36.374682
1450.214083	174358.467331	36.379700
1451.215756	174648.689435	36.384717
1452.990959	174930.815649	36.389735
1454.224102	175207.423720	36.394752
1455.757174	175514.898865	36.399770
1457.272272	175800.601159	36.404788
1458.681678	176087.312481	36.409805
1460.351824	176384.871382	36.414823
1461.699610	176677.979955	36.419840
1462.892373	176958.653025	36.424858
1464.720054	177255.251948	36.429876
1466.378432	177554.469658	36.434893
1467.823750	177845.106818	36.439911
1469.373906	178133.431152	36.444928
1470.735726	178432.055800	36.449946
1472.331466	178724.995729	36.454964
1473.702385	179027.442577	36.459981
1475.072525	179315.092607	36.464999
1476.448324	179623.088512	36.470016
1478.073734	179921.335607	36.475034
1479.547083	180234.636996	36.480052
1480.764761	180536.800710	36.485069
1482.418147	180840.328401	36.490087
1483.875629	181161.621401	36.495104
1485.164292	181473.424955	36.500122
1487.086324	181782.054113	36.505140
1488.088254	182101.244995	36.510157
1489.951219	182399.898462	36.515175
1491.392010	182721.355978	36.520192
1492.727747	183036.752938	36.525210
1494.583042	183351.418557	36.530228
1495.767239	183669.458975	36.535245
1497.297073	183975.690426	36.540263
1499.142449	184305.112465	36.545280
1500.653492	184610.322433	36.550298
1502.339538	184939.368420	36.555316
1503.462720	185261.515364	36.560333
1505.296715	185560.622514	36.565351
1506.697156	185885.646728	36.570368
1508.008553	186205.902087	36.575386
1509.711948	186513.578632	36.580404
1511.191266	186845.018300	36.585421
1512.766686	187151.703964	36.590439
1514.353197	187462.438762	36.595456
1515.846540	187782.812581	36.600474
1517.630234	188100.918772	36.605492
1518.804905	188425.575892	36.610509
1520.612129	188729.959439	36.615527
1521.779857	189056.169898	36.620544
1523.702802	189364.675918	36.625562
1525.144163	189682.301445	36.630580
1526.586596	190000.779021	36.635597
1528.054842	190305.658332	36.640615
1529.769640	190626.696606	36.645632
1531.268150	190935.953722	36.650650
1533.042637	191241.079165	36.655668
1534.450844	191535.780876	36.660685
1536.065921	191817.996314	36.665703
1537.499420	192119.539124	36.670720
1538.829286	192407.631311	36.675738
1540.957582	192701.978462	36.680756
1542.405975	192996.388570	36.685773
1543.360994	193283.505783	36.690791
1545.084805	193581.313502	36.695808
1546.346114	193890.992839	36.700826
1548.195810	194188.325611	36.705844
1549.459519	194497.588584	36.710861
1550.848620	194804.356754	36.715879
1552.750050	195115.320095	36.720896
1554.031888	195429.027965	36.725914
1555.803795	195723.968601	36.730932
1557.134620	196035.360735	36.735949
1558.575344	196347.434459	36.740967
1560.498884	196665.066786	36.745984
1561.877812	196979.451644	36.751002
1563.548016	197291.695062	36.756020
1565.065719	197610.617779	36.761037
1566.495799	197928.566211	36.766055
1568.270693	198249.214208	36.771072
1569.702304	198575.227393	36.776090
1571.435967	198899.567136	36.781108
1572.604744	199228.953255	36.786125
1574.070823	199556.946034	36.791143
1575.743845	199885.426728	36.796160
1577.199388	200234.500306	36.801178
1579.350155	200571.640401	36.806196
1580.495466	200902.054041	36.811213
1582.391541	201232.180134	36.816231
1584.071207	201565.162159	36.821248
1585.311958	201903.030281	36.826266
1587.275387	202232.159525	36.831284
1588.563932	202576.574410	36.836301
1590.594662	202913.872352	36.841319
1592.210393	203247.837643	36.846336
1593.556035	203579.804861	36.851354
1595.439181	203916.687384	36.856372
1596.789356	204258.166938	36.861389
1598.563168	204605.139396	36.866407
1599.855849	204952.700823	36.871424
1601.000768	205293.507925	36.876442
1603.134424	205635.727661	36.881460
1604.878024	205989.555250	36.886477
1606.178453	206333.515599	36.891495
1607.916193	206684.211057	36.896512
1609.563786	207041.830425	36.901530
1610.967718	207387.416268	36.906548
1612.702377	207739.932669	36.911565
1614.506607	208088.248889	36.916583
1616.355070	208441.270168	36.921600
1617.917166	208799.520990	36.926618
1619.479033	209142.053475	36.931636
1620.877568	209505.362743	36.936653
1622.548215	209849.022995	36.941671
1624.034073	210196.042065	36.946688
1625.790094	210553.328759	36.951706
1627.440406	210901.796532	36.956724
1628.778187	211265.047232	36.961741
1630.493392	211617.037278	36.966759
1632.314565	211972.312797	36.971776
1634.049978	212333.038810	36.976794
1635.860644	212679.658669	36.981812
1637.331907	213037.459771	36.986829
1638.639001	213384.444925	36.991847
1640.544180	213733.567550	36.996864
1642.046829	214070.465796	37.001882
1643.876193	214412.289166	37.006900
1645.557127	214741.922207	37.011917
1647.203983	215069.098498	37.016935
1648.899392	215407.138042	37.021952
1649.991725	215742.306904	37.026970
1651.839087	216075.625175	37.031988
1653.375889	216422.304341	37.037005
1654.936080	216767.533208	37.042023
1656.761484	217112.186128	37.047040
1658.157310	217460.695529	37.052058
1659.912656	217808.562606	37.057076
1661.270463	218177.729481	37.062093
1662.990045	218521.693609	37.067111
1664.468404	218885.458705	37.072128
1665.933582	219246.763611	37.077146
1667.711288	219613.758229	37.082164
1669.198896	219974.934963	37.087181
1670.776199	220350.143628	37.092199
1672.749173	220727.345557	37.097216
1674.039175	221109.436628	37.102234
1676.132969	221479.458720	37.107252
1677.616010	221859.183812	37.112269
1679.350451	222240.138633	37.117287
1680.945503	222623.200514	37.122304
1682.442528	223028.986920	37.127322
1683.910696	223472.142142	37.132340
1685.872906	223866.094692	37.137357
1687.644030	224267.674622	37.142375
1689.264156	224648.554676	37.147392
1690.743942	225047.899378	37.152410
1692.687781	225442.622155	37.157428
1694.119005	225851.324660	37.162445
1695.691958	226257.236487	37.167463
1697.461180	226655.751159	37.172480
1699.426738	227064.369329	37.177498
1700.930093	227464.479839	37.182516
1702.578135	227879.909495	37.187533
1704.432569	228300.716653	37.192551
1706.324722	228712.755713	37.197568
1707.699184	229118.582180	37.202586
1709.535298	229535.332073	37.207604
1711.098616	229954.211127	37.212621
1712.959560	230377.334990	37.217639
1714.831798	230787.351360	37.222656
1716.228907	231207.887158	37.227674
1718.006213	231627.472305	37.232692
1720.215947	232057.706458	37.237709
1721.800979	232479.916624	37.242727
1723.477859	232898.785196	37.247744
1724.783584	233315.049041	37.252762
1726.604572	233742.913485	37.257780
1728.615550	234174.557880	37.262797
1730.082682	234605.835995	37.267815
1732.165106	235026.497316	37.272832
1733.792435	235463.669693	37.277850
1735.588962	235875.896136	37.282868
1737.365556	236309.286484	37.287885
1738.561706	236744.069226	37.292903
1740.714721	237168.559579	37.297920
1742.449726	237597.133430	37.302938
1744.631756	238020.604795	37.307956
1745.838949	238455.237169	37.312973
1747.661255	238889.819677	37.317991
1749.631310	239315.005300	37.323008
1751.625890	239750.348608	37.328026
1753.199369	240167.142496	37.333044
1755.284941	240579.407183	37.338061
1756.785871	240994.233215	37.343079
1758.803070	241397.619849	37.348096
1760.278315	241793.247334	37.353114
1761.766987	242202.539775	37.358132
1763.792836	242605.926989	37.363149
1765.211888	243022.217951	37.368167
1767.227436	243417.911161	37.373184
1768.814429	243838.951353	37.378202
1770.882246	244247.541671	37.383220
1772.564653	244667.195604	37.388237
1774.405984	245081.717939	37.393255
1776.084964	245490.069382	37.398272
1777.548664	245907.805151	37.403290
1779.624360	246329.327015	37.408308
1781.433849	246744.314040	37.413325
1783.098803	247173.271629	37.418343
1785.271552	247588.148850	37.423360
1786.736455	248025.294826	37.428378
1788.330107	248444.333107	37.433396
1790.393568	248874.446152	37.438413
1792.175344	249318.425415	37.443431
1794.107028	249733.751117	37.448448
1795.659784	250170.630787	37.453466
1797.532173	250605.146379	37.458484
1799.278555	251033.891239	37.463501
1800.913568	251479.979781	37.468519
1803.127880	251914.846407	37.473536
1805.015310	252358.836267	37.478554
1806.657841	252800.809218	37.483572
1808.549936	253234.764620	37.488589
1809.830447	253685.638216	37.493607
1811.895429	254126.475231	37.498624
1813.737741	254585.055304	37.503642
1815.655605	255043.978753	37.508660
1817.598738	255490.094962	37.513677
1819.204182	255943.075175	37.518695
1821.516511	256385.243990	37.523712
1823.165789	256848.073686	37.528730
1825.337212	257300.224063	37.533748
1826.935995	257751.935611	37.538765
1828.482984	258202.512607	37.543783
1830.913099	258651.292558	37.548800
1832.334023	259115.531968	37.553818
1834.100351	259574.481226	37.558836
1836.171872	260022.634436	37.563853
1837.967823	260487.396037	37.568871
1839.776064	260940.520802	37.573888
1841.684896	261415.856709	37.578906
1843.474278	261873.379092	37.583924
1845.317630	262326.980291	37.588941
1847.042000	262790.635239	37.593959
1849.097107	263261.170429	37.598976
1851.080831	263718.837722	37.603994
1852.614349	264181.989988	37.609012
1854.762499	264638.994496	37.614029
1856.553243	265115.745182	37.619047
1858.848033	265569.219184	37.624064
1860.667670	266030.417650	37.629082
1862.314693	266491.390205	37.634100
1864.408947	266954.066708	37.639117
1866.077250	267411.072026	37.644135
1868.278950	267869.995646	37.649152
1870.005525	268329.403702	37.654170
1871.794904	268789.004108	37.659188
1873.502772	269249.404940	37.664205
1875.477910	269709.430845	37.669223
1877.657129	270168.711192	37.674240
1879.174988	270632.520258	37.679258
1880.365272	271063.181298	37.684276
1882.488064	271516.016829	37.689293
1884.695837	271956.822177	37.694311
1886.582918	272392.700918	37.699328
1888.264562	272844.819852	37.704346
1890.041238	273288.971355	37.709364
1891.657220	273734.876062	37.714381
1893.371275	274188.257591	37.719399
1895.669337	274641.592699	37.724416
1897.236766	275113.870878	37.729434
1898.585469	275569.799722	37.734452
1900.704267	276025.981567	37.739469
1902.715362	276504.864575	37.744487
1904.400849	276981.691961	37.749504
1906.490227	277457.232321	37.754522
1908.064005	277939.029504	37.759540
1910.195361	278410.420266	37.764557
1911.915794	278902.758274	37.769575
1913.976917	279383.557132	37.774592
1915.681823	279881.559920	37.779610
1917.634576	280359.046611	37.784628
1920.035101	280842.503767	37.789645
1921.767010	281346.264413	37.794663
1923.973873	281837.269805	37.799680
1925.859083	282333.915284	37.804698
1927.694918	282830.516680	37.809716
1929.974283	283318.432297	37.814733
1931.544005	283828.283399	37.819751
1933.645285	284331.237587	37.824768
1935.639606	284826.993912	37.829786
1937.382740	285329.089608	37.834804
1939.383275	285828.575649	37.839821
1941.085410	286344.975510	37.844839
1943.502788	286842.408041	37.849856
1945.201140	287363.046863	37.854874
1947.147505	287874.879602	37.859892
1949.604073	288382.714531	37.864909
1951.544895	288893.604597	37.869927
1953.208669	289400.957024	37.874944
1955.353669	289922.553795	37.879962
1957.158301	290439.505654	37.884980
1959.366253	290951.689824	37.889997
1961.555518	291471.113987	37.895015
1963.643259	291973.103051	37.900032
1965.957252	292481.936027	37.905050
1967.545266	292996.576247	37.910068
1969.505607	293501.627939	37.915085
1971.618883	294012.367066	37.920103
1973.507851	294518.797689	37.925120
1975.454978	295037.509659	37.930138
1977.314846	295546.785185	37.935156
1979.563740	296060.769132	37.940173
1981.190278	296577.774283	37.945191
1983.336704	297086.665117	37.950208
1985.709207	297611.136307	37.955226
1987.555776	298131.500966	37.960244
1989.925174	298633.083512	37.965261
1991.732832	299150.350837	37.970279
1993.784735	299662.089195	37.975296
1995.904416	300170.867569	37.980314
1997.476624	300692.584991	37.985332
1999.774280	301197.061802	37.990349
2001.562026	301716.350718	37.995367
2003.604831	302224.394425	38.000384
2005.722827	302737.527808	38.005402
2007.667533	303249.518690	38.010420
2010.000838	303757.988557	38.015437
2012.048758	304261.778875	38.020455
2013.927932	304749.340339	38.025472
2015.805073	305233.166159	38.030490
2017.426930	305720.917107	38.035508
2019.605429	306201.183091	38.040525
2021.556020	306694.029698	38.045543
2023.417640	307190.037234	38.050560
2025.670049	307675.869784	38.055578
2027.265166	308175.115352	38.060596
2030.141076	308678.971575	38.065613
2031.677633	309176.874746	38.070631
2033.980814	309665.886930	38.075648
2035.948082	310165.236576	38.080666
2037.726745	310674.289661	38.085684
2039.813342	311166.248747	38.090701
2041.516769	311682.316620	38.095719
2043.688024	312179.613527	38.100736
2045.632391	312703.989485	38.105754
2047.656139	313216.769013	38.110772
2049.839456	313745.389840	38.115789
2051.800364	314263.759174	38.120807
2053.455612	314792.104165	38.125824
2055.943169	315315.711711	38.130842
2057.588135	315851.363932	38.135860
2059.856110	316385.690411	38.140877
2061.488938	316928.471919	38.145895
2063.998774	317462.191646	38.150912
2066.283024	318002.800440	38.155930
2068.152962	318559.267290	38.160948
2070.468697	319090.644944	38.165965
2072.703008	319641.558093	38.170983
2074.909024	320175.484450	38.176000
2076.993113	320720.954292	38.181018
2078.937575	321266.366483	38.186036
2081.531381	321808.213744	38.191053
2083.070446	322352.007935	38.196071
2084.860503	322896.187708	38.201088
2087.382908	323443.212569	38.206106
2089.512909	324009.670035	38.211124
2091.310125	324559.597773	38.216141
2093.922281	325113.169128	38.221159
2095.679196	325675.585217	38.226176
2097.902898	326224.513607	38.231194
2099.825214	326793.366232	38.236212
2102.147719	327346.761884	38.241229
2104.191765	327901.721649	38.246247
2106.232670	328472.544285	38.251264
2108.071492	329028.136585	38.256282
2110.518242	329592.686584	38.261300
2112.789542	330155.736757	38.266317
2114.901619	330715.532715	38.271335
2117.008911	331295.785751	38.276352
2118.837033	331866.685826	38.281370
2121.052255	332430.484122	38.286388
2123.435935	332991.177138	38.291405
2125.441053	333564.035960	38.296423
2127.756249	334140.137687	38.301440
2130.028336	334688.545020	38.306458
2132.266867	335264.038121	38.311476
2134.464267	335819.731671	38.316493
2136.463194	336394.388973	38.321511
2138.500822	336963.652135	38.326528
2140.683389	337519.127050	38.331546
2142.881138	338094.113525	38.336564
2145.520240	338639.880577	38.341581
2147.429856	339214.724331	38.346599
2149.126029	339779.189834	38.351616
2151.441436	340343.952895	38.356634
2153.498900	340903.041137	38.361652
2156.186669	341449.404188	38.366669
2158.357877	341991.836138	38.371687
2160.184243	342520.562273	38.376704
2162.595291	343058.729443	38.381722
2164.568068	343588.866471	38.386740
2166.700025	344126.458631	38.391757
2168.638624	344660.269605	38.396775
2170.425368	345208.870784	38.401792
2172.604241	345749.152442	38.406810
2174.148578	346311.790330	38.411828
2176.529780	346867.608569	38.416845
2178.511585	347438.231112	38.421863
2180.533036	347995.338678	38.426880
2182.969664	348571.023839	38.431898
2184.839110	349145.044239	38.436916
2187.222944	349717.906557	38.441933
2189.004394	350298.245727	38.446951
2191.115921	350894.180336	38.451968
2193.624291	351475.551428	38.456986
2195.696370	352075.968188	38.462004
2197.789187	352669.318787	38.467021
2200.291833	353268.429964	38.472039
2202.441748	353874.949798	38.477056
2204.581762	354482.147784	38.482074
2206.549524	355095.835988	38.487092
2208.907520	355698.159439	38.492109
2210.934104	356303.015563	38.497127
2213.076671	356931.669247	38.502144
2215.386132	357536.308496	38.507162
2217.875542	358161.613112	38.512180
2219.842313	358773.547230	38.517197
2222.350707	359398.398430	38.522215
2224.753064	360031.731489	38.527232
2227.092866	360640.937145	38.532250
2229.188999	361277.497782	38.537268
2231.733357	361902.151749	38.542285
2234.126439	362533.391545	38.547303
2236.269748	363169.076658	38.552320
2238.591069	363784.046370	38.557338
2240.578209	364419.381632	38.562356
2243.061969	365046.912546	38.567373
2245.394443	365681.510342	38.572391
2247.544558	366303.926014	38.577408
2250.164370	366941.676932	38.582426
2252.327395	367579.949016	38.587444
2254.761241	368203.453255	38.592461
2256.876972	368843.131998	38.597479
2258.892704	369481.370359	38.602496
2261.358563	370112.776344	38.607514
2263.769103	370748.974371	38.612532
2265.679682	371381.642114	38.617549
2267.933408	372023.930912	38.622567
2270.295796	372675.498440	38.627584
2272.542003	373305.058709	38.632602
2274.979186	373951.847757	38.637620
2277.399795	374604.181842	38.642637
2279.791422	375240.784775	38.647655
2282.190480	375886.149605	38.652672
2284.309832	376517.854172	38.657690
2286.508539	377159.703272	38.662708
2288.856813	377802.606127	38.667725
2291.386270	378436.160355	38.672743
2293.672219	379091.525599	38.677760
2295.723671	379719.885565	38.682778
2297.877646	380361.351880	38.687796
2300.212324	381007.619186	38.692813
2302.380640	381643.226422	38.697831
2304.669376	382291.099085	38.702848
2306.999780	382905.635352	38.707866
2309.283407	383529.447636	38.712884
2311.763262	384149.108193	38.717901
2313.891575	384767.623287	38.722919
2315.980296	385372.797215	38.727936
2318.540259	385988.124493	38.732954
2321.045433	386603.778532	38.737972
2323.114454	387233.714996	38.742989
2325.446516	387855.508426	38.748007
2327.573767	388492.609908	38.753024
2330.205091	389118.055500	38.758042
2332.350448	389748.283796	38.763060
2334.530821	390390.331607	38.768077
2336.807295	391024.872320	38.773095
2339.051072	391674.259363	38.778112
2341.059489	392310.363919	38.783130
2343.434552	392972.628938	38.788148
2345.823749	393628.819296	38.793165
2348.077510	394291.759739	38.798183
2349.849631	394945.716670	38.803200
2352.581190	395617.977346	38.808218
2354.898468	396292.926958	38.813236
2357.093611	396967.475791	38.818253
2359.904739	397648.167232	38.823271
2361.889118	398329.258019	38.828288
2364.306971	399015.684498	38.833306
2366.939603	399711.511566	38.838324
2369.361205	400393.444584	38.843341
2371.744160	401079.270128	38.848359
2373.922301	401781.051522	38.853376
2376.412434	402468.320913	38.858394
2378.999112	403170.988640	38.863412
2381.416169	403876.225882	38.868429
2383.740648	404574.898334	38.873447
2385.773546	405278.187235	38.878464
2388.488376	405987.628992	38.883482
2390.902100	406692.921887	38.888500
2392.979710	407410.944628	38.893517
2395.528701	408121.067907	38.898535
2397.771901	408845.510911	38.903552
2399.921118	409566.707460	38.908570
2402.747763	410283.111853	38.913588
2404.883532	411021.573040	38.918605
2407.643142	411743.800747	38.923623
2409.759927	412476.702618	38.928640
2412.726574	413197.437991	38.933658
2414.793615	413932.409823	38.938676
2417.244879	414656.913313	38.943693
2419.993085	415387.096794	38.948711
2422.230592	416128.158164	38.953728
2424.779467	416852.963954	38.958746
2427.265835	417590.548490	38.963764
2429.570769	418329.433161	38.968781
2432.217068	419057.021858	38.973799
2434.557366	419798.744682	38.978816
2436.937957	420536.336885	38.983834
2439.290352	421281.533609	38.988852
2441.674910	422017.612820	38.993869
2444.234351	422745.412534	38.998887
2446.837508	423490.678775	39.003904
2449.284516	424232.150512	39.008922
2452.160177	424971.199883	39.013940
2454.344309	425705.075143	39.018957
2456.730988	426440.616241	39.023975
2459.168706	427190.049652	39.028992
2461.444380	427925.259968	39.034010
2464.374868	428670.363694	39.039028
2466.264768	429396.884612	39.044045
2469.070746	430105.108969	39.049063
2471.355024	430811.525163	39.054080
2473.669143	431519.383214	39.059098
2476.182523	432232.147642	39.064116
2478.628956	432945.458131	39.069133
2480.993998	433656.279980	39.074151
2483.021576	434381.914996	39.079168
2485.547375	435098.942054	39.084186
2488.152986	435834.102857	39.089204
2490.030020	436554.683525	39.094221
2492.536952	437296.291455	39.099239
2494.843712	438050.002969	39.104256
2497.281257	438787.170728	39.109274
2499.893279	439547.107294	39.114292
2502.177360	440304.795115	39.119309
2504.682919	441067.278142	39.124327
2506.922700	441831.853303	39.129344
2509.406537	442603.596910	39.134362
2512.020324	443392.291522	39.139380
2514.533981	444169.489863	39.144397
2516.835428	444958.381848	39.149415
2519.593310	445741.301614	39.154432
2522.100733	446543.052521	39.159450
2524.735589	447331.600542	39.164468
2526.766163	448137.417376	39.169485
2529.618636	448940.792046	39.174503
2532.082450	449751.129767	39.179520
2534.718232	450553.467497	39.184538
2537.382458	451369.273498	39.189556
2539.656212	452190.220062	39.194573
2542.625584	453003.838505	39.199591
2544.993167	453831.026325	39.204608
2547.660964	454645.944920	39.209626
2550.371547	455460.217461	39.214644
2552.695665	456290.347678	39.219661
2555.810165	457109.190383	39.224679
2557.993005	457943.574305	39.229696
2560.926883	458772.895967	39.234714
2563.667156	459600.547180	39.239732
2566.180824	460428.757769	39.244749
2568.949011	461251.837039	39.249767
2571.193773	462095.541876	39.254784
2574.320643	462927.692409	39.259802
2576.927555	463753.676744	39.264820
2579.167313	464598.539154	39.269837
2582.229094	465418.363931	39.274855
2584.826976	466263.449116	39.279872
2587.241984	467103.170966	39.284890
2590.248952	467922.292734	39.289908
2592.455539	468766.928912	39.294925
2594.911608	469598.248200	39.299943
2597.518222	470445.220323	39.304960
2599.986673	471283.992606	39.309978
2602.951571	472125.677230	39.314996
2605.700498	472972.462490	39.320013
2608.394799	473803.810747	39.325031
2611.231524	474642.423366	39.330048
2613.820663	475473.613704	39.335066
2616.915815	476301.551723	39.340084
2619.118832	477151.975225	39.345101
2622.038739	477969.513150	39.350119
2624.513482	478802.693899	39.355136
2627.221431	479632.566132	39.360154
2630.001540	480456.833738	39.365172
2632.342722	481296.487484	39.370189
2635.332569	482121.856699	39.375207
2637.722475	482954.558002	39.380224
2640.410429	483764.602392	39.385242
2642.995106	484563.418801	39.390260
2645.577638	485361.997815	39.395277
2648.161912	486139.388046	39.400295
2651.100828	486943.491164	39.405312
2653.263395	487724.414876	39.410330
2655.917390	488525.161108	39.415348
2658.411044	489335.033016	39.420365
2661.224086	490122.859307	39.425383
2663.926152	490934.590837	39.430400
2666.314538	491736.696800	39.435418
2668.895984	492533.232950	39.440436
2671.126384	493364.912095	39.445453
2673.820983	494183.405126	39.450471
2676.046433	495013.642491	39.455488
2678.722110	495852.695645	39.460506
2681.679838	496687.624517	39.465524
2684.164501	497539.238698	39.470541
2686.894930	498382.092244	39.475559
2689.257265	499232.732671	39.480576
2691.849048	500102.258301	39.485594
2695.089083	500957.205775	39.490612
2697.335532	501837.844707	39.495629
2700.024572	502705.099418	39.500647
2703.010017	503589.961104	39.505664
2705.369677	504466.002730	39.510682
2708.158947	505348.532373	39.515700
2710.998291	506240.182995	39.520717
2714.026565	507118.694417	39.525735
2716.359547	508022.179275	39.530752
2719.109253	508908.453918	39.535770
2722.132029	509795.088245	39.540788
2724.714675	510708.614289	39.545805
2727.531359	511605.969558	39.550823
2730.495573	512509.348580	39.555840
2733.078721	513413.293207	39.560858
2736.028174	514313.295254	39.565876
2738.864152	515231.860183	39.570893
2741.444263	516134.338202	39.575911
2744.556253	517044.738466	39.580928
2746.942697	517971.630888	39.585946
2750.089451	518876.879051	39.590964
2752.993392	519794.709113	39.595981
2755.576114	520704.678386	39.600999
2758.561499	521619.715632	39.606016
2761.298026	522538.315304	39.611034
2764.496963	523450.587819	39.616052
2767.200753	524372.456333	39.621069
2769.857979	525288.131953	39.626087
2772.874298	526198.606241	39.631104
2775.575026	527121.162583	39.636122
2778.208011	528041.407127	39.641140
2780.892831	528962.139957	39.646157
2783.564553	529883.673561	39.651175
2786.512588	530795.790487	39.656192
2789.316713	531727.305868	39.661210
2792.273966	532650.129112	39.666228
2794.774793	533580.318011	39.671245
2797.748598	534515.050151	39.676263
2800.340119	535433.629957	39.681280
2803.336265	536367.936705	39.686298
2806.143150	537287.872548	39.691316
2809.274569	538222.187330	39.696333
2812.090235	539146.681793	39.701351
2815.304755	540085.489730	39.706368
2817.572000	541009.349764	39.711386
2820.862422	541924.479255	39.716404
2823.492030	542853.340223	39.721421
2826.769830	543756.028858	39.726439
2829.495219	544637.073349	39.731456
2831.974845	545510.810459	39.736474
2835.177658	546397.699855	39.741492
2837.387513	547279.164892	39.746509
2840.307666	548155.227249	39.751527
2843.113678	549030.649368	39.756544
2845.519104	549924.281499	39.761562
2848.541177	550819.060680	39.766580
2851.221899	551717.054684	39.771597
2853.759736	552600.687254	39.776615
2856.788723	553504.085129	39.781632
2859.301484	554425.550690	39.786650
2862.405930	555331.577982	39.791668
2865.182675	556258.050760	39.796685
2867.791471	557170.819485	39.801703
2870.475077	558098.938674	39.806720
2873.205670	559038.993063	39.811738
2876.154630	559984.671890	39.816756
2878.754501	560943.250797	39.821773
2881.435241	561886.275531	39.826791
2884.726441	562840.533368	39.831808
2887.211136	563815.245236	39.836826
2890.232095	564772.670921	39.841844
2893.279035	565760.101042	39.846861
2895.833157	566734.180737	39.851879
2898.668492	567709.546367	39.856896
2902.003188	568702.528021	39.861914
2904.846825	569682.712603	39.866932
2907.586707	570677.596885	39.871949
2910.450619	571681.919572	39.876967
2913.725842	572675.254201	39.881984
2916.283916	573691.663814	39.887002
2919.586184	574687.395066	39.892020
2922.476440	575700.877843	39.897037
2925.261219	576699.043509	39.902055
2928.651250	577712.381095	39.907072
2931.470709	578732.351880	39.912090
2934.506082	579737.455999	39.917108
2937.425377	580765.368688	39.922125
2940.293702	581780.716114	39.927143
2943.493356	582800.739075	39.932160
2946.326387	583817.026771	39.937178
2949.575131	584840.782373	39.942196
2952.811415	585863.250498	39.947213
2955.923598	586888.710716	39.952231
2959.069012	587913.426658	39.957248
2961.972011	588936.842199	39.962266
2964.915552	589945.829888	39.967284
2968.013624	590963.727399	39.972301
2971.035127	591991.772892	39.977319
2974.146308	592997.167182	39.982336
2977.004458	594024.612312	39.987354
2980.389628	595039.507168	39.992372
2983.390809	596062.091925	39.997389
2986.213115	597078.255767	40.002407
2989.434814	598087.654320	40.007424
2992.273182	599122.368640	40.012442
2995.639404	600128.411146	40.017460
2998.378677	601140.928610	40.022477
3001.295364	602160.837830	40.027495
3004.601777	603162.720322	40.032512
3007.685712	604186.727230	40.037530
3010.790042	605196.173756	40.042548
3013.367511	606214.726446	40.047565
3015.983422	607233.882034	40.052583
3019.283254	608242.875277	40.057600
3022.248503	609265.893199	40.062618
3025.545206	610273.854416	40.067636
3028.508997	611258.868083	40.072653
3031.391026	612237.655792	40.077671
3034.402572	613201.331060	40.082688
3037.132945	614176.622081	40.087706
3040.074432	615144.841288	40.092724
3043.185617	616121.348319	40.097741
3045.741011	617116.210202	40.102759
3049.192348	618101.185242	40.107776
3052.190885	619096.544315	40.112794
3054.960465	620086.551885	40.117812
3057.999708	621091.719216	40.122829
3061.198739	622097.816607	40.127847
3064.314112	623095.189087	40.132864
3066.854638	624116.298579	40.137882
3070.010475	625130.514727	40.142900
3072.702741	626160.448058	40.147917
3075.704192	627198.323569	40.152935
3078.793735	628226.093896	40.157952
3081.511703	629285.739722	40.162970
3084.825316	630324.207374	40.167988
3087.858230	631394.576398	40.173005
3090.457339	632454.972454	40.178023
3093.850696	633525.464515	40.183040
3096.900769	634605.887208	40.188058
3099.949520	635686.148307	40.193076
3103.042205	636771.580134	40.198093
3105.878832	637869.715472	40.203111
3109.141257	638956.287464	40.208128
3112.290247	640061.023851	40.213146
3115.460186	641159.801273	40.218164
3119.044536	642266.273612	40.223181
3121.721094	643377.613535	40.228199
3124.880094	644495.584713	40.233216
3127.600499	645612.158619	40.238234
3131.078644	646731.725132	40.243252
3134.412781	647851.440270	40.248269
3137.732469	648981.152065	40.253287
3141.084873	650109.185925	40.258304
3144.034837	651247.923315	40.263322
3147.403126	652366.429530	40.268340
3150.388417	653500.766963	40.273357
3153.851315	654640.276049	40.278375
3156.966441	655763.023212	40.283392
3160.129468	656911.285249	40.288410
3162.906720	658051.906410	40.293428
3166.397102	659199.995222	40.298445
3169.071873	660348.879730	40.303463
3172.549473	661491.073745	40.308480
3175.444440	662669.716492	40.313498
3178.820290	663822.353926	40.318516
3181.941710	664972.556090	40.323533
3184.994260	666133.777896	40.328551
3188.334542	667294.363361	40.333568
3191.865873	668462.039148	40.338586
3194.669164	669613.674384	40.343604
3198.206014	670790.961055	40.348621
3201.081881	671960.103837	40.353639
3204.191933	673120.709157	40.358656
3207.656944	674296.872746	40.363674
3210.985325	675463.366331	40.368692
3214.227753	676628.236924	40.373709
3217.056629	677819.717789	40.378727
3220.456468	678981.036559	40.383744
3224.034287	680161.507774	40.388762
3227.208528	681336.230632	40.393780
3230.457555	682498.869201	40.398797
3233.487622	683686.477893	40.403815
3236.450534	684833.867014	40.408832
3239.884134	685970.804984	40.413850
3243.222490	687106.523805	40.418868
3246.443615	688233.034777	40.423885
3249.608037	689372.418847	40.428903
3252.944475	690485.078355	40.433920
3255.868684	691607.244941	40.438938
3258.977652	692752.957069	40.443956
3262.119557	693887.899767	40.448973
3264.977326	695039.510510	40.453991
3267.943895	696177.909392	40.459008
3271.303794	697348.083085	40.464026
3274.323759	698522.223221	40.469044
3277.674281	699683.112840	40.474061
3280.631210	700870.384459	40.479079
3283.835538	702063.748481	40.484096
3287.042617	703249.812061	40.489114
3290.165215	704450.493567	40.494132
3293.678425	705656.592020	40.499149
3296.812988	706865.407769	40.504167
3300.401334	708093.889795	40.509184
3303.538109	709310.335133	40.514202
3306.697060	710545.667197	40.519220
3309.969698	711773.127554	40.524237
3313.246877	713022.784340	40.529255
3316.486117	714259.790435	40.534272
3319.987835	715522.107097	40.539290
3323.031039	716768.179709	40.544308
3326.562254	718025.761102	40.549325
3330.008383	719296.918469	40.554343
3333.081143	720565.915803	40.559360
3336.763373	721834.866175	40.564378
3339.731619	723102.404909	40.569396
3343.164628	724391.374050	40.574413
3345.913648	725676.695430	40.579431
3350.003826	726968.068347	40.584448
3353.341415	728268.304749	40.589466
3356.560357	729556.150970	40.594484
3360.128814	730856.627677	40.599501
3363.523544	732168.629039	40.604519
3366.888473	733464.423541	40.609536
3370.496314	734766.832120	40.614554
3373.692055	736090.816993	40.619572
3376.965980	737383.673995	40.624589
3380.168523	738711.270731	40.629607
3383.889736	740024.054979	40.634624
3387.342269	741349.344019	40.639642
3390.472714	742668.446696	40.644660
3393.945658	743981.305206	40.649677
3397.192583	745310.005813	40.654695
3400.589561	746640.280277	40.659712
3404.284248	747977.869455	40.664730
3407.419432	749302.803820	40.669748
3410.978895	750634.340067	40.674765
3414.737138	751977.634521	40.679783
3418.469930	753310.503465	40.684800
3421.483204	754644.589488	40.689818
3425.208644	755976.848809	40.694836
3428.875497	757308.196234	40.699853
3431.888409	758641.584362	40.704871
3435.044476	759963.592955	40.709888
3438.634020	761306.702510	40.714906
3442.118198	762653.673474	40.719924
3445.677817	763984.799107	40.724941
3449.157092	765321.258672	40.729959
3452.483950	766666.108825	40.734976
3455.998894	767999.919580	40.739994
3459.437342	769340.384551	40.745012
3462.892294	770649.148509	40.750016
3466.300693	771919.319625	40.755021
3469.663116	773150.913423	40.760026
3472.877253	774316.783747	40.765031
3475.932991	775407.756121	40.770036
3479.043267	776425.994573	40.775040
3481.864386	777381.676280	40.780045
3484.346577	778272.815942	40.785050
3487.491334	779103.947023	40.790055
3489.798016	779866.135862	40.795060
3492.578619	780570.454779	40.800064
3494.927949	781203.836031	40.805069
3496.973693	781763.128896	40.810074
3499.019547	782270.386212	40.815079
3500.927648	782719.985321	40.820084
3502.762679	783100.761853	40.825088
3504.278004	783472.964311	40.830093
3506.307254	783772.082623	40.835098
3507.691552	784018.971040	40.840103
3509.015407	784224.898125	40.845108
3510.832076	784379.941440	40.850112
3511.603700	784509.042658	40.855117
3512.761972	784585.512452	40.860122
3514.505744	784631.644025	40.865127
3514.975447	784646.170846	40.870132
3516.320972	784629.968192	40.875136
3516.838257	784574.367193	40.880141
3517.163966	784500.799945	40.885146
3517.892245	784399.136523	40.890151
3518.932811	784278.832171	40.895156
3519.641196	784131.238859	40.900160
3520.596313	783975.192626	40.905165
3521.089142	783780.663587	40.910170
3521.525493	783574.728930	40.915175
3521.647849	783359.003898	40.920180
3522.354834	783107.420268	40.925184
3522.587511	782862.988554	40.930189
3522.751379	782585.998580	40.935194
3523.271225	782308.742542	40.940199
3523.415678	782027.208951	40.945204
3524.170391	781727.805446	40.950208
3524.016127	781418.552844	40.955213
3524.452317	781088.133596	40.960218
3524.525051	780762.777395	40.965223
3524.326797	780434.302328	40.970228
3524.460422	780085.584290	40.975232
3524.635880	779755.442312	40.980237
3524.788986	779387.005134	40.985242
3525.125046	779039.482788	40.990247
3524.585065	778680.867595	40.995252
3524.724232	778301.550727	41.000256
3524.819472	777943.729558	41.005261
3524.901278	777574.916850	41.010266
3524.994370	777202.391871	41.015271
3524.742607	776833.202764	41.020276
3525.029373	776458.491148	41.025280
3525.130222	776075.520196	41.030285
3525.056589	775693.739501	41.035290
3524.749050	775301.637896	41.040295
3524.118780	774926.703383	41.045300
3524.894674	774539.355481	41.050304
3524.533770	774165.420905	41.055309
3524.206090	773771.517159	41.060314
3524.094522	773389.425582	41.065319
3524.152741	773009.009945	41.070324
3524.105649	772622.287500	41.075328
3523.841016	772245.185552	41.080333
3523.937346	771853.719753	41.085338
3523.737788	771475.976603	41.090343
3523.875238	771103.183500	41.095348
3524.066971	770707.897130	41.100352
3523.576644	770331.227183	41.105357
3523.646516	769957.648396	41.110362
3523.361962	769573.515233	41.115367
3523.184342	769189.640192	41.120372
3523.325241	768817.174839	41.125376
3523.095407	768438.295990	41.130381
3523.068985	768064.341994	41.135386
3523.078906	767681.688758	41.140391
3522.390222	767304.207734	41.145396
3522.496455	766918.640633	41.150400
3522.353922	766564.544238	41.155405
3522.204273	766186.622022	41.160410
3522.398589	765822.033323	41.165415
3522.030399	765458.850658	41.170420
3522.056392	765090.704333	41.175424
3521.735644	764731.718671	41.180429
3521.895953	764365.437499	41.185434
3522.058999	763994.354823	41.190439
3521.603056	763639.086747	41.195444
3521.455420	763272.161878	41.200448
3521.236981	762916.524601	41.205453
3521.213896	762574.746653	41.210458
3521.097243	762212.795668	41.215463
3520.870761	761867.714529	41.220468
3521.033082	761514.710510	41.225472
3520.730543	761167.982092	41.230477
3520.243180	760814.953740	41.235482
3520.472159	760475.555064	41.240487
3519.896827	760137.951119	41.245492
3519.794621	759782.196278	41.250496
3519.646021	759465.066154	41.255501
3519.403527	759120.750388	41.260506
3519.398183	758780.179490	41.265511
3519.168478	758459.911979	41.270516
3519.152813	758137.917831	41.275520
3519.266574	757823.883631	41.280525
3519.042370	757495.283577	41.285530
3519.018913	757166.488202	41.290535
3518.684825	756841.135502	41.295540
3518.728586	756526.072198	41.300544
3518.386294	756226.213523	41.305549
3518.167320	755908.305048	41.310554
3518.174601	755587.137300	41.315559
3518.485339	755277.310021	41.320564
3518.404988	754973.014683	41.325568
3518.086416	754666.277927	41.330573
3518.048775	754359.630728	41.335578
3517.931255	754047.009986	41.340583
3517.559713	753743.158206	41.345588
3517.242323	753437.902857	41.350592
3517.556908	753142.160643	41.355597
3517.150129	752845.340723	41.360602
3517.036252	752552.016833	41.365607
3516.892134	752245.747324	41.370612
3516.849685	751961.081316	41.375616
3516.690737	751671.731868	41.380621
3516.184981	751380.255438	41.385626
3516.723229	751111.613834	41.390631
3516.096982	750838.807910	41.395636
3516.332363	750553.698487	41.400640
3516.500460	750274.221231	41.405645
3516.153056	749981.480395	41.410650
3515.969953	749708.166392	41.415655
3515.983145	749434.859818	41.420660
3516.082330	749157.280458	41.425664
3515.720986	748885.992550	41.430669
3515.307554	748610.701509	41.435674
3515.475221	748349.832124	41.440679
3515.432233	748076.437615	41.445684
3515.306671	747814.215009	41.450688
3515.092055	747560.250901	41.455693
3514.873378	747296.444866	41.460698
3514.906877	747043.955039	41.465703
3514.884215	746789.390576	41.470708
3514.546763	746511.294616	41.475712
3514.445836	746268.884305	41.480717
3514.094188	746015.238478	41.485722
3514.639900	745768.900258	41.490727
3514.127845	745530.093636	41.495732
3514.050897	745270.941136	41.500736
3514.075837	745040.236727	41.505741
3513.777716	744791.683476	41.510746
3513.770933	744552.566072	41.515751
3513.858433	744322.077418	41.520756
3513.779009	744073.860901	41.525760
3513.741036	743841.846224	41.530765
3513.514300	743602.340617	41.535770
3513.314443	743372.711991	41.540775
3512.842872	743154.197089	41.545780
3513.189070	742902.610125	41.550784
3512.888108	742691.669026	41.555789
3512.799661	742468.226088	41.560794
3512.906324	742244.942476	41.565799
3512.443488	742023.971722	41.570804
3512.703863	741804.804296	41.575808
3512.333137	741595.427892	41.580813
3512.416081	741380.333210	41.585818
3512.394286	741155.803586	41.590823
3511.920595	740944.102403	41.595828
3512.244677	740726.675123	41.600832
3511.914282	740523.446204	41.605837
3511.917763	740326.240953	41.610842
3511.866911	740114.398460	41.615847
3511.877386	739916.390444	41.620852
3511.875366	739708.585208	41.625856
3511.683707	739499.519620	41.630861
3511.156974	739300.941692	41.635866
3511.266131	739090.529583	41.640871
3510.953065	738907.737085	41.645876
3511.020841	738710.728480	41.650880
3511.414329	738532.758208	41.655885
3510.768522	738342.883342	41.660890
3510.892737	738151.442263	41.665895
3510.628408	737959.120539	41.670900
3510.494073	737768.652936	41.675904
3510.616834	737583.333784	41.680909
3510.796972	737410.321573	41.685914
3510.887104	737216.983420	41.690919
3510.263776	737039.741162	41.695924
3510.498763	736855.772160	41.700928
3510.425881	736679.272437	41.705933
3510.059498	736504.796631	41.710938
3510.400759	736320.748328	41.715943
3510.091590	736146.750161	41.720948
3510.296164	735954.995765	41.725952
3510.082823	735806.214107	41.730957
3509.728495	735615.434507	41.735962
3509.830375	735444.124889	41.740967
3509.641956	735286.965192	41.745972
3509.851493	735109.889417	41.750976
3509.580849	734951.301343	41.755981
3509.402064	734790.319151	41.760986
3508.904661	734632.207609	41.765991
3509.020304	734465.181147	41.770996
3509.309139	734307.676154	41.776000
3509.320188	734150.263351	41.781005
3509.024787	733989.036823	41.786010
3509.089651	733846.063714	41.791015
3508.896915	733684.022116	41.796020
3508.929374	733519.959966	41.801024
3508.704899	733376.630162	41.806029
3508.999608	733223.608007	41.811034
3508.973108	733074.447948	41.816039
3508.917231	732926.379155	41.821044
3508.735510	732767.238304	41.826048
3508.419649	732622.325855	41.831053
3508.644326	732464.745915	41.836058
3508.384156	732317.392770	41.841063
3508.081575	732175.539863	41.846068
3508.430444	732039.370236	41.851072
3508.219788	731891.753603	41.856077
3508.134312	731756.542048	41.861082
3508.156276	731613.932596	41.866087
3508.143334	731480.140446	41.871092
3507.957357	731329.736532	41.876096
3508.062335	731206.616337	41.881101
3508.067311	731077.667434	41.886106
3507.998766	730922.680806	41.891111
3507.710375	730786.099909	41.896116
3507.587834	730654.491129	41.901120
3507.608050	730532.810815	41.906125
3507.614837	730394.589953	41.911130
3507.608427	730259.389916	41.916135
3507.610780	730132.456932	41.921140
3507.752873	730015.453697	41.926144
3507.557334	729875.622981	41.931149
3507.238419	729759.831147	41.936154
3507.210504	729635.668942	41.941159
3507.222576	729512.290719	41.946164
3507.306612	729382.707523	41.951168
3507.228268	729250.078113	41.956173
3507.110064	729123.000646	41.961178
3507.457107	729015.706975	41.966183
3506.811128	728907.436260	41.971188
3507.253350	728784.223793	41.976192
3507.110372	728662.690991	41.981197
3506.813814	728546.977286	41.986202
3507.116323	728426.853616	41.991207
3507.209624	728295.963682	41.996212
3506.853376	728181.245355	42.001216
3506.658783	728071.650725	42.006221
3506.873008	727954.061080	42.011226
3507.116299	727833.888906	42.016231
3506.495255	727728.323084	42.021236
3506.516925	727611.949204	42.026240
3506.611306	727498.682796	42.031245
3506.188451	727392.832274	42.036250
3506.619398	727273.314529	42.041255
3506.218263	727178.951576	42.046260
3506.622307	727073.753367	42.051264
3506.528727	726967.149463	42.056269
3506.352528	726850.252360	42.061274
3506.288894	726744.631531	42.066279
3505.851516	726635.652205	42.071284
3506.042103	726529.392152	42.076288
3506.046274	726445.408427	42.081293
3506.183830	726345.397747	42.086298
3506.221162	726236.632184	42.091303
3505.787203	726134.879792	42.096308
3505.797037	726029.584490	42.101312
3506.030910	725936.737748	42.106317
3505.903951	725844.147619	42.111322
3505.800987	725737.727476	42.116327
3505.770331	725647.101337	42.121332
3505.567170	725558.980281	42.126336
3505.578308	725465.421615	42.131341
3505.334739	725371.606527	42.136346
3505.555672	725286.286813	42.141351
3505.592167	725196.090628	42.146356
3505.792922	725087.481138	42.151360
3505.501344	724999.814656	42.156365
3505.378292	724907.510665	42.161370
3505.627358	724815.144323	42.166375
3505.533650	724732.893730	42.171380
3505.666361	724632.714326	42.176384
3505.667965	724539.890084	42.181389
3505.434624	724445.269795	42.186394
3505.597216	724350.087574	42.191399
3505.234073	724273.576235	42.196404
3505.209079	724180.901013	42.201408
3505.513435	724102.692134	42.206413
3504.860721	724022.608156	42.211418
3505.624393	723927.123760	42.216423
3505.296978	723858.830131	42.221428
3505.224117	723754.461037	42.226432
3505.493838	723670.950423	42.231437
3505.399700	723584.128498	42.236442
3505.404884	723486.533562	42.241447
3505.076448	723412.932885	42.246452
3505.377155	723314.791565	42.251456
3504.948579	723245.369491	42.256461
3504.604570	723151.297824	42.261466
3505.036551	723066.763013	42.266471
3505.005649	722993.159136	42.271476
3505.053811	722906.504914	42.276480
3505.297693	722828.194795	42.281485
3505.236424	722750.330776	42.286490
3505.080923	722664.104133	42.291495
3504.687642	722587.235125	42.296500
3504.826344	722495.604577	42.301504
3504.904945	722424.852749	42.306509
3504.900970	722353.866060	42.311514
3504.985255	722277.113770	42.316519
3504.925335	722203.408502	42.321524
3505.023590	722120.505366	42.326528
3504.943380	722036.738469	42.331533
3504.953096	721955.781672	42.336538
3504.955497	721880.030691	42.341543
3504.839469	721792.102902	42.346548
3504.721087	721727.326664	42.351552
3504.967900	721653.714694	42.356557
3504.434370	721572.595783	42.361562
3504.717384	721497.340416	42.366567
3504.491628	721425.836969	42.371572
3504.412083	721341.715894	42.376576
3504.405614	721278.752115	42.381581
3504.216394	721217.503664	42.386586
3504.453206	721135.212378	42.391591
3504.090873	721063.034192	42.396596
3504.494939	721002.182196	42.401600
3504.372084	720933.086990	42.406605
3503.809835	720867.088070	42.411610
3504.447377	720789.685461	42.416615
3504.213984	720739.547069	42.421620
3504.288629	720678.052832	42.426624
3504.368702	720611.598966	42.431629
3504.196922	720528.823591	42.436634
3504.638662	720473.564434	42.441639
3504.013826	720407.076333	42.446644
3504.394346	720332.934790	42.451648
3504.526070	720264.932525	42.456653
3504.119324	720196.720919	42.461658
3504.560460	720120.832015	42.466663
3504.254258	720068.718143	42.471668
3504.210000	719989.238651	42.476672
3504.151043	719925.826995	42.481677
3504.099956	719858.000290	42.486682
3503.930742	719789.944558	42.491687
3504.120521	719728.969803	42.496692
3504.355882	719660.300880	42.501696
3504.316085	719596.586030	42.506701
3504.183251	719526.290651	42.511706
3504.175779	719463.214116	42.516711
3504.104508	719405.404157	42.521716
3504.089603	719341.187353	42.526720
3504.092553	719285.496720	42.531725
3504.229760	719210.492654	42.536730
3504.264868	719143.290615	42.541735
3503.770901	719092.986871	42.546740
3503.856026	719017.245771	42.551744
3504.190108	718958.622040	42.556749
3504.035895	718906.029515	42.561754
3504.294373	718834.324815	42.566759
3503.932473	718766.391665	42.571764
3504.529223	718703.457796	42.576768
3504.220292	718641.119038	42.581773
3504.083517	718568.634078	42.586778
3504.304551	718500.453927	42.591783
3503.913921	718449.286150	42.596788
3503.920075	718371.766766	42.601792
3504.130935	718315.737831	42.606797
3503.892109	718258.493100	42.611802
3504.205591	718193.866185	42.616807
3503.981474	718137.510951	42.621812
3503.969769	718072.688696	42.626816
3503.982544	718017.781559	42.631821
3504.095107	717958.244951	42.636826
3504.089899	717883.252440	42.641831
3503.669212	717828.663480	42.646836
3503.694888	717764.328671	42.651840
3503.613972	717721.785356	42.656845
3503.787251	717652.514965	42.661850
3503.404734	717601.787065	42.666855
3503.295003	717553.940368	42.671860
3503.679641	717497.381312	42.676864
3503.678163	717450.359408	42.681869
3503.451544	717397.471713	42.686874
3503.645121	717339.554221	42.691879
3503.802172	717286.056978	42.696884
3503.430814	717229.521480	42.701888
3503.756790	717161.957976	42.706893
3503.716439	717118.016018	42.711898
3503.717064	717064.543138	42.716903
3503.730268	717002.783938	42.721908
3503.605679	716951.662369	42.726912
3503.746864	716895.436999	42.731917
3503.098026	716845.095632	42.736922
3503.450041	716777.574349	42.741927
3503.325249	716744.061510	42.746932
3503.698315	716686.754813	42.751936
3503.662221	716623.959220	42.756941
3503.481549	716585.345486	42.761946
3503.498810	716526.905765	42.766951
3503.362639	716486.151138	42.771956
3503.486859	716422.335475	42.776960
3503.482186	716375.258464	42.781965
3503.340129	716319.919247	42.786970
3503.481173	716270.436440	42.791975
3503.354219	716221.592808	42.796980
3503.317792	716160.282069	42.801985
3503.451297	716113.081603	42.806989
3503.423966	716057.572925	42.811994
3503.522764	716006.160741	42.816999
3503.471824	715963.901232	42.822004
3503.549036	715903.413271	42.827009
3503.376659	715848.968942	42.832013
3503.185430	715808.071264	42.837018
3503.814481	715754.288048	42.842023
3503.317191	715710.662076	42.847028
3503.138779	715664.056218	42.852033
3503.527759	715623.111648	42.857037
3503.220481	715570.027276	42.862042
3503.406388	715511.651936	42.867047
3503.379952	715470.130104	42.872052
3503.622468	715420.972876	42.877057
3503.640663	715358.506180	42.882061
3503.304780	715309.592449	42.887066
3503.432289	715258.419039	42.892071
3503.615171	715211.155766	42.897076
3503.444057	715156.756365	42.902081
3503.798364	715105.346194	42.907085
3503.279860	715057.304551	42.912090
3503.477068	715012.816285	42.917095
3503.210397	714963.492211	42.922100
3503.518637	714904.844429	42.927105
3503.384048	714860.062714	42.932109
3503.242409	714808.335518	42.937114
3503.547925	714763.282301	42.942119
3503.281812	714706.910951	42.947124
3503.156971	714656.172409	42.952129
3503.714948	714611.821057	42.957133
3503.444092	714550.884555	42.962138
3503.528421	714490.385279	42.967143
3503.485122	714449.605484	42.972148
3503.403505	714398.659794	42.977153
3503.460810	714353.645292	42.982157
3502.887537	714306.005345	42.987162
3503.319415	714244.454636	42.992167
3503.029655	714206.939612	42.997172
3503.076005	714155.673645	43.002177
3503.429534	714120.781397	43.007181
3502.797246	714073.447587	43.012186
3503.290204	714035.554722	43.017191
3503.120678	713986.258545	43.022196
3503.088113	713940.313830	43.027201
3503.203243	713888.637932	43.032205
3503.062773	713847.871243	43.037210
3503.347036	713797.804475	43.042215
3503.512337	713760.857586	43.047220
3502.977436	713702.737377	43.052225
3503.249775	713653.763442	43.057229
3503.314044	713610.927291	43.062234
3503.256122	713558.682401	43.067239
3502.802476	713516.179232	43.072244
3503.295001	713473.718444	43.077249
3503.298483	713423.100225	43.082253
3503.141564	713381.142988	43.087258
3502.940983	713334.180527	43.092263
3503.326912	713290.346861	43.097268
3503.051917	713241.559982	43.102273
3503.127275	713200.853863	43.107277
3502.962729	713168.822150	43.112282
3503.165651	713114.695346	43.117287
3503.073551	713076.696088	43.122292
3502.805234	713023.341131	43.127297
3503.484385	712976.876890	43.132301
3503.088306	712941.160370	43.137306
3502.981315	712891.450482	43.142311
3502.975458	712839.639231	43.147316
3503.045418	712807.766026	43.152321
3502.945340	712756.069047	43.157325
3502.697157	712729.657555	43.162330
3502.983015	712677.499470	43.167335
3503.021281	712640.767147	43.172340
3503.173056	712603.420401	43.177345
3502.694626	712557.343126	43.182349
3502.770129	712520.008580	43.187354
3503.321492	712470.981836	43.192359
3502.829909	712442.872474	43.197364
3503.016090	712390.282368	43.202369
3503.070420	712349.774153	43.207373
3502.762015	712309.176619	43.212378
3503.099715	712265.295974	43.217383
3502.853989	712222.106825	43.222388
3503.016943	712187.734349	43.227393
3503.113936	712141.014036	43.232397
3502.940018	712105.555180	43.237402
3503.421270	712057.976965	43.242407
3503.152323	712008.189320	43.247412
3503.252488	711962.212004	43.252417
3503.309360	711915.894135	43.257421
3502.892544	711876.999957	43.262426
3503.140786	711821.120231	43.267431
3503.278798	711793.202779	43.272436
3503.209979	711738.863803	43.277441
3503.200873	711699.157101	43.282445
3502.866683	711663.027909	43.287450
3503.183919	711615.226066	43.292455
3502.964176	711571.185513	43.297460
3503.277241	711526.113846	43.302465
3503.097685	711479.286554	43.307469
3502.870631	711443.386958	43.312474
3502.994483	711395.466834	43.317479
3503.013324	711358.136519	43.322484
3502.844299	711312.001494	43.327489
3503.012300	711269.980271	43.332493
3502.944920	711232.067955	43.337498
3503.030041	711182.117848	43.342503
3502.815347	711151.973041	43.347508
3502.788459	711103.629365	43.352513
3502.874847	711067.428339	43.357517
3502.756371	711031.856587	43.362522
3502.823065	710975.554471	43.367527
3502.753860	710941.711611	43.372532
3502.448402	710899.915496	43.377537
3502.799968	710863.421707	43.382541
3502.656941	710839.915781	43.387546
3502.753444	710808.626390	43.392551
3502.685442	710780.143874	43.397556
3502.456048	710732.774635	43.402561
3502.796733	710695.140175	43.407565
3502.596368	710663.849527	43.412570
3502.439833	710616.417994	43.417575
3502.419020	710586.288877	43.422580
3502.586791	710548.533337	43.427585
3502.571351	710518.750590	43.432589
3502.707728	710484.822397	43.437594
3502.774153	710445.246327	43.442599
3502.648205	710411.857496	43.447604
3502.950184	710373.135850	43.452609
3502.697763	710331.278560	43.457613
3502.684418	710302.239363	43.462618
3502.663445	710255.379206	43.467623
3502.312226	710219.594192	43.472628
3502.389386	710187.908558	43.477633
3502.600661	710147.562575	43.482637
3502.515199	710120.073619	43.487642
3502.838088	710074.148698	43.492647
3502.960018	710045.135981	43.497652
3502.580507	710002.602987	43.502657
3502.645198	709980.996631	43.507661
3502.772798	709945.677669	43.512666
3502.821820	709907.988508	43.517671
3502.817839	709868.024195	43.522676
3502.536147	709825.474199	43.527681
3502.552217	709780.591184	43.532685
3502.376982	709758.229452	43.537690
3502.418008	709715.029969	43.542695
3502.529100	709688.400880	43.547700
3502.920483	709656.860088	43.552705
3502.647388	709604.874580	43.557709
3502.626478	709570.323252	43.562714
3503.071454	709540.163338	43.567719
3502.653629	709504.435945	43.572724
3502.848862	709459.670667	43.577729
3502.625229	709421.527802	43.582733
3502.332566	709398.539044	43.587738
3502.901340	709349.888681	43.592743
3502.645618	709326.744695	43.597748
3502.516538	709286.351431	43.602753
3502.864350	709248.361880	43.607757
3502.431051	709213.231614	43.612762
3502.965584	709173.373917	43.617767
3502.519600	709150.608355	43.622772
3502.806243	709102.152024	43.627777
3502.890215	709067.978588	43.632781
3502.213525	709047.137492	43.637786
3502.767363	708997.941432	43.642791
3502.247385	708975.982015	43.647796
3502.211081	708941.579636	43.652801
3502.912294	708906.062560	43.657805
3502.628793	708878.006418	43.662810
3502.899286	708826.274165	43.667815
3502.546669	708797.831931	43.672820
3502.373775	708762.458293	43.677825
3502.568305	708725.286120	43.682829
3502.310498	708688.982767	43.687834
3502.609874	708667.582687	43.692839
3502.465869	708625.649516	43.697844
3502.415131	708595.816228	43.702849
3502.667705	708563.400522	43.707853
3502.571529	708532.233850	43.712858
3502.567174	708497.079613	43.717863
3502.638138	708469.559572	43.722868
3502.547684	708430.049675	43.727873
3502.357033	708386.980969	43.732877
3502.342226	708356.892655	43.737882
3502.579238	708318.023450	43.742887
3501.953126	708309.337703	43.747892
3502.533274	708283.272471	43.752897
3502.688208	708250.275807	43.757901
3502.286626	708204.956789	43.762906
3502.646992	708165.570012	43.767911
3502.584004	708144.178680	43.772916
3502.648967	708109.756273	43.777921
3502.364543	708071.021527	43.782925
3502.401056	708035.312439	43.787930
3502.407725	708004.673126	43.792935
3502.145117	707977.603726	43.797940
3502.373926	707947.573147	43.802945
3502.448812	707925.860609	43.807949
3502.385992	707900.297422	43.812954
3502.590013	707859.842539	43.817959
3502.541072	707837.405315	43.822964
3502.619252	707797.318478	43.827969
3502.609166	707757.792240	43.832973
3502.300333	707726.012119	43.837978
3502.890578	707689.217180	43.842983
3502.578366	707648.846366	43.847988
3503.005756	707613.667025	43.852993
3502.864374	707580.815932	43.857997
3502.425038	707537.535638	43.863002
3502.793365	707505.345162	43.868007
3502.801353	707484.784707	43.873012
3502.643473	707442.003813	43.878017
3502.546799	707405.718131	43.883021
3502.471605	707371.812464	43.888026
3502.834529	707326.263506	43.893031
3502.469605	707304.721190	43.898036
3502.316255	707282.498363	43.903041
3502.652317	707235.215212	43.908045
3502.555106	707209.208682	43.913050
3502.488156	707173.910353	43.918055
3502.570187	707127.661703	43.923060
3502.400116	707105.639821	43.928065
3502.668325	707067.157114	43.933069
3502.350848	707033.786658	43.938074
3502.374268	707002.247083	43.943079
3502.358626	706968.528662	43.948084
3502.294745	706938.046158	43.953089
3502.569949	706910.835108	43.958093
3502.276983	706886.349753	43.963098
3502.290212	706850.341596	43.968103
3502.264875	706825.762305	43.973108
3502.430127	706798.022716	43.978113
3502.567542	706764.476931	43.983117
3502.373485	706737.342656	43.988122
3502.419284	706699.639918	43.993127
3502.244235	706674.389562	43.998132
3502.109779	706645.407586	44.003137
3502.385867	706598.577804	44.008141
3502.221409	706586.983317	44.013146
3502.520794	706541.738670	44.018151
3502.368424	706517.378092	44.023156
3502.441587	706484.239126	44.028161
3502.415956	706457.821202	44.033165
3502.190949	706431.883044	44.038170
3502.319166	706395.953371	44.043175
3502.563233	706369.242405	44.048180
3502.446782	706334.197117	44.053185
3502.688427	706302.668687	44.058189
3502.204731	706284.173049	44.063194
3502.344118	706239.151845	44.068199
3502.434720	706213.210689	44.073204
3502.348293	706177.067136	44.078209
3502.347758	706148.856100	44.083213
3502.429190	706124.406217	44.088218
3502.288160	706084.496522	44.093223
3502.320969	706056.031348	44.098228
3502.164360	706018.507985	44.103233
3502.567841	705999.964885	44.108237
3502.120444	705965.966001	44.113242
3502.211590	705928.103408	44.118247
3502.150663	705909.139948	44.123252
3502.319288	705871.065662	44.128257
3502.658329	705849.950059	44.133261
3502.410317	705830.470891	44.138266
3502.049988	705795.115909	44.143271
3502.175977	705767.131125	44.148276
3502.103753	705742.109439	44.153281
3502.757287	705706.686374	44.158285
3502.178609	705681.300932	44.163290
3502.651082	705655.493857	44.168295
3502.394508	705623.200641	44.173300
3502.022358	705605.430220	44.178305
3502.412274	705560.761561	44.183309
3502.236914	705537.941801	44.188314
3502.442219	705495.538425	44.193319
3502.369002	705477.569468	44.198324
3502.553441	705441.974258	44.203329
3502.404155	705408.371095	44.208333
3502.459415	705383.426706	44.213338
3502.696898	705351.349096	44.218343
3502.694604	705317.969722	44.223348
3502.212994	705285.215596	44.228353
3502.201582	705228.441555	44.233357
3502.061326	705228.812415	44.238362
3502.536160	705176.577491	44.243367
3502.212207	705165.752468	44.248372
3502.126753	705123.891911	44.253377
3502.528786	705104.602030	44.258381
3502.387300	705076.808104	44.263386
3502.531557	705042.360366	44.268391
3502.397336	705003.885094	44.273396
3502.356144	704979.501848	44.278401
3502.587857	704953.881378	44.283405
3502.513526	704937.600414	44.288410
3502.441670	704889.825203	44.293415
3502.157755	704862.401780	44.298420
3502.538024	704831.043838	44.303425
3502.401218	704797.138188	44.308429
3502.359581	704773.102161	44.313434
3502.649837	704734.506070	44.318439
3502.533466	704712.071812	44.323444
3502.343706	704670.921710	44.328449
3502.683408	704640.314904	44.333453
3502.512758	704606.116024	44.338458
3502.588676	704563.580368	44.343463
3502.935825	704542.907333	44.348468
3502.491020	704502.046837	44.353473
3502.923664	704459.551244	44.358477
3502.645615	704427.157737	44.363482
3502.716100	704391.875049	44.368487
3502.606947	704361.440574	44.373492
3502.527017	704329.163087	44.378497
3502.826240	704285.794422	44.383501
3502.585423	704252.152166	44.388506
3502.486853	704208.948020	44.393511
3502.550400	704190.705458	44.398516
3502.710298	704159.977547	44.403521
3502.622647	704113.939421	44.408525
3502.352939	704091.429460	44.413530
3502.624504	704055.367075	44.418535
3502.575981	704013.693778	44.423540
3502.360517	703990.926218	44.428545
3502.342620	703951.483175	44.433549
3502.273162	703937.286095	44.438554
3502.603449	703889.935903	44.443559
3502.497989	703861.088840	44.448564
3502.353958	703829.316860	44.453569
3502.702417	703790.011440	44.458573
3502.569941	703765.540452	44.463578
3502.777371	703727.748428	44.468583
3502.373552	703691.050593	44.473588
3502.421475	703671.020969	44.478593
3502.374821	703637.940513	44.483597
3502.224329	703597.027244	44.488602
3502.249578	703572.181945	44.493607
3502.044108	703535.252037	44.498612
3502.379398	703517.857570	44.503617
3502.452746	703484.110878	44.508621
3502.413743	703466.529569	44.513626
3502.376135	703428.230103	44.518631
3502.305770	703405.288044	44.523636
3502.486709	703373.361479	44.528641
3502.374095	703338.054987	44.533645
3502.723732	703317.527678	44.538650
3502.229542	703278.706579	44.543655
3502.123446	703251.149377	44.548660
3502.193333	703222.320979	44.553665
3502.708833	703192.027890	44.558669
3502.329237	703172.812830	44.563674
3502.293869	703130.139424	44.568679
3502.544503	703100.982730	44.573684
3502.291712	703072.753542	44.578689
3502.194289	703031.729491	44.583693
3502.247155	703007.474251	44.588698
3502.589361	702976.662425	44.593703
3502.232928	702954.014740	44.598708
3502.322638	702920.610964	44.603713
3502.537278	702887.236161	44.608717
3502.604341	702862.034135	44.613722
3502.663339	702814.126544	44.618727
3502.414602	702780.082382	44.623732
3502.505813	702759.745401	44.628737
3502.465902	702721.343822	44.633741
3502.346669	702696.718575	44.638746
3502.329041	702650.015203	44.643751
3502.281296	702626.421418	44.648756
3502.252141	702604.364833	44.653761
3502.560882	702570.724871	44.658765
3502.133683	702550.522511	44.663770
3502.357981	702521.119772	44.668775
3502.382740	702499.302479	44.673780
3502.111153	702465.608669	44.678785
3502.291414	702433.728454	44.683789
3502.293598	702411.517149	44.688794
3502.486056	702379.435969	44.693799
3502.219645	702344.101089	44.698804
3502.315698	702331.116344	44.703809
3502.301007	702287.143463	44.708813
3502.176870	702269.623448	44.713818
3502.345784	702233.719490	44.718823
3502.411809	702206.826274	44.723828
3502.307167	702182.942520	44.728833
3502.405694	702146.950421	44.733837
3502.082949	702123.201822	44.738842
3502.257103	702078.053881	44.743847
3502.563504	702060.363120	44.748852
3502.620104	702038.936955	44.753857
3502.604871	701993.173795	44.758861
3502.305264	701971.905542	44.763866
3502.562241	701923.016282	44.768871
3502.704212	701882.891509	44.773876
3502.314941	701873.116652	44.778881
3502.669881	701819.092375	44.783885
3502.166967	701799.695822	44.788890
3502.318319	701762.003881	44.793895
3502.400564	701719.999874	44.798900
3502.440432	701704.340030	44.803905
3502.434684	701678.152712	44.808909
3502.254596	701658.255409	44.813914
3502.352916	701618.335384	44.818919
3502.017955	701601.345698	44.823924
3502.203427	701567.771870	44.828929
3502.437896	701535.034640	44.833933
3502.102018	701517.150447	44.838938
3502.134922	701486.583096	44.843943
3502.079533	701454.986602	44.848948
3502.203413	701427.584503	44.853953
3502.317881	701390.940625	44.858957
3502.343859	701370.213590	44.863962
3502.530698	701340.117311	44.868967
3502.116840	701314.393709	44.873972
3502.278243	701294.439305	44.878977
3502.376330	701251.933478	44.883981
3502.050407	701242.793516	44.888986
3502.193617	701201.770881	44.893991
3502.283843	701177.703172	44.898996
3502.407262	701141.205859	44.904001
3502.665508	701105.083749	44.909005
3502.057188	701073.378196	44.914010
3501.984333	701048.989127	44.919015
3502.433579	701028.986687	44.924020
3502.129986	700999.069438	44.929025
3501.834529	700961.397966	44.934029
3502.013318	700953.615757	44.939034
3501.789182	700921.796650	44.944039
3501.950977	700920.179707	44.949044
3502.016423	700878.820486	44.954049
3502.241001	700858.457093	44.959053
3501.837280	700834.022547	44.964058
3502.096854	700812.858113	44.969063
3501.927710	700791.068494	44.974068
3501.717685	700764.961793	44.979073
3502.170561	700752.512285	44.984077
3502.043648	700726.143280	44.989082
3502.135671	700695.762214	44.994087
3502.001814	700664.573378	44.999092
3502.116053	700654.714180	45.004097
3501.946759	700625.320210	45.009101
3501.994457	700603.345294	45.014106
3502.031502	700574.662644	45.019111
3502.106799	700548.408882	45.024116
3502.128113	700516.796352	45.029121
3501.957779	700497.789389	45.034125
3501.609164	700482.887167	45.039130
3502.023806	700451.010788	45.044135
3501.788963	700445.532795	45.049140
3501.626545	700427.915983	45.054145
3501.928020	700383.086198	45.059149
3501.949630	700384.971299	45.064154
3502.020436	700344.304474	45.069159
3502.090624	700327.096439	45.074164
3501.912837	700301.430347	45.079169
3501.885744	700274.944130	45.084173
3502.005403	700262.747640	45.089178
3501.921048	700223.795666	45.094183
3502.146818	700208.152208	45.099188
3501.943771	700186.813983	45.104193
3502.390071	700152.992935	45.109197
3502.256564	700126.822015	45.114202
3502.079021	700102.745767	45.119207
3502.162435	700075.942525	45.124212
3502.010013	700056.235816	45.129217
3502.260567	700024.583734	45.134221
3502.166083	700014.360587	45.139226
3502.094726	699985.743571	45.144231
3502.098599	699965.215657	45.149236
3502.120370	699942.050481	45.154241
3502.141174	699913.169525	45.159245
3502.107097	699888.124683	45.164250
3502.277832	699855.988110	45.169255
3502.463267	699830.956638	45.174260
3502.233360	699807.882281	45.179265
3502.444641	699776.981334	45.184269
3502.294338	699744.599028	45.189274
3502.301553	699708.562222	45.194279
3502.232406	699683.124937	45.199284
3502.035249	699667.550204	45.204289
3502.210353	699636.952953	45.209293
3502.455876	699610.966559	45.214298
3502.433492	699562.656884	45.219303
3502.154462	699549.381875	45.224308
3502.097980	699514.547695	45.229313
3502.243133	699493.100695	45.234317
3502.147908	699466.374729	45.239322
3502.486550	699444.547787	45.244327
3502.364007	699392.625143	45.249332
3502.094465	699375.421511	45.254337
3502.149616	699345.091539	45.259341
3502.207113	699316.103156	45.264346
3502.194185	699291.003415	45.269351
3502.349902	699265.627279	45.274356
3501.942802	699245.662467	45.279361
3502.170765	699211.028746	45.284365
3502.234520	699190.837102	45.289370
3502.077481	699162.132098	45.294375
3502.227018	699141.876498	45.299380
3502.191968	699119.613248	45.304385
3502.371319	699084.539668	45.309389
3502.050705	699070.624579	45.314394
3502.528293	699031.177041	45.319399
3502.045151	699005.656880	45.324404
3502.158035	698983.816285	45.329409
3502.393781	698943.264905	45.334413
3502.332468	698931.742598	45.339418
3502.249131	698898.103407	45.344423
3501.916740	698880.163521	45.349428
3501.604943	698853.869046	45.354433
3501.896293	698823.398932	45.359437
3501.715103	698811.051159	45.364442
3501.938790	698776.366719	45.369447
3502.015982	698758.011125	45.374452
3501.768456	698739.112480	45.379457
3502.280284	698712.085346	45.384461
3502.374015	698693.478342	45.389466
3502.122143	698671.697074	45.394471
3502.278076	698638.812828	45.399476
3501.849542	698625.213076	45.404481
3502.143757	698589.422643	45.409485
3502.041544	698548.477731	45.414490
3501.915598	698544.471929	45.419495
3502.184308	698513.706206	45.424500
3501.921478	698491.230338	45.429505
3502.249403	698452.997940	45.434509
3502.198573	698442.566918	45.439514
3502.046619	698403.220297	45.444519
3502.369705	698384.723982	45.449524
3501.907972	698355.817986	45.454529
3502.145607	698332.314716	45.459533
3501.962960	698312.708489	45.464538
3501.905242	698298.351153	45.469543
3501.812465	698263.020860	45.474548
3501.783036	698250.846141	45.479553
3501.956752	698220.393322	45.484557
3501.724271	698193.387817	45.489562
3501.935473	698175.008924	45.494567
3502.272254	698155.018476	45.499572
3501.810325	698136.203572	45.504577
3502.095638	698107.372514	45.509581
3501.998338	698094.562487	45.514586
3501.939548	698071.057650	45.519591
3501.998515	698033.315170	45.524596
3501.786566	698023.506767	45.529601
3502.168925	697993.863922	45.534605
3501.786363	697979.808164	45.539610
3501.879963	697946.384742	45.544615
3502.031624	697923.888838	45.549620
3502.167922	697911.288624	45.554625
3501.855320	697888.173123	45.559629
3501.761723	697863.878031	45.564634
3501.617202	697837.751807	45.569639
3501.912605	697806.034627	45.574644
3501.970446	697803.290797	45.579649
3502.242087	697774.610048	45.584653
3501.991534	697753.770878	45.589658
3501.705577	697732.390619	45.594663
3502.133930	697703.236375	45.599668
3501.810892	697690.711534	45.604673
3502.038029	697648.514980	45.609677
3501.847639	697648.148661	45.614682
3501.816466	697622.947728	45.619687
3502.036523	697592.783400	45.624692
3501.770598	697580.547289	45.629697
3501.806443	697542.259632	45.634701
3501.813476	697530.326492	45.639706
3501.933652	697510.817727	45.644711
3501.827767	697477.723699	45.649716
3501.904017	697469.607285	45.654721
3502.159529	697447.739375	45.659725
3501.855794	697441.873108	45.664730
3501.966947	697411.228930	45.669735
3501.817984	697374.860261	45.674740
3501.552895	697373.760474	45.679745
3502.057808	697343.498638	45.684749
3502.122725	697333.295817	45.689754
3502.025980	697296.470758	45.694759
3502.074548	697277.420740	45.699764
3501.913522	697259.001836	45.704769
3502.193883	697227.881675	45.709773
3501.969748	697212.058433	45.714778
3501.761386	697177.886355	45.719783
3502.070482	697159.041745	45.724788
3501.996102	697128.476876	45.729793
3502.114685	697111.055689	45.734797
3501.945957	697083.091604	45.739802
3501.821906	697062.180230	45.744807
3501.939872	697049.283490	45.749812
3501.845755	697021.207475	45.754817
3502.201763	696973.716172	45.759821
3501.951776	696900.121887	45.764826
3501.763276	696758.498601	45.769831
3501.869706	696570.831532	45.774836
3501.367441	696323.294329	45.779841
3501.714525	696017.431810	45.784845
3501.330451	695669.808932	45.789850
3500.998308	695247.420506	45.794855
3500.766611	694775.661092	45.799860
3500.496470	694249.870615	45.804865
3500.143125	693648.112195	45.809869
3499.893253	693029.930880	45.814874
3499.489818	692313.135831	45.819879
3498.804144	691555.285822	45.824884
3498.393939	690741.053667	45.829889
3497.804813	689858.805507	45.834893
3497.334631	688936.042128	45.839898
3496.919349	687941.854552	45.844903
3496.237354	686898.771231	45.849908
3495.155779	685790.419146	45.854913
3494.956776	684624.579408	45.859917
3493.958494	683407.034824	45.864922
3492.909721	682111.645057	45.869927
3492.276236	680773.864954	45.874932
3490.977446	679369.095729	45.879937
3490.430648	677916.007440	45.884941
3489.404902	676406.658330	45.889946
3488.403824	674834.509407	45.894951
3487.653632	673215.793731	45.899956
3486.261652	671527.151959	45.904961
3485.137115	669783.508012	45.909965
3484.039158	667993.102501	45.914970
3482.548151	666146.900313	45.919975
3481.352532	664243.160686	45.924980
3480.265399	662290.615952	45.929985
3478.632939	660285.902041	45.934989
3477.893418	658220.214124	45.939994
3476.541575	656104.351176	45.944999
3474.978506	653937.567920	45.950004
3473.048961	651728.002933	45.955009
3472.100882	649459.017605	45.960013
3470.071853	647142.561008	45.965018
3468.807424	644776.449769	45.970023
3467.199323	642359.785377	45.975028
3465.344277	639914.728562	45.980033
3463.813776	637397.291250	45.985037
3461.826775	634850.541627	45.990042
3460.163043	632259.767908	45.995047
3458.428121	629604.679417	46.000052
3456.483063	626920.613466	46.005057
3454.532627	624188.033125	46.010061
3452.597407	621420.432609	46.015066
3450.529366	618599.722010	46.020071
3448.520472	615736.813924	46.025076
3446.580883	612840.455904	46.030081
3444.541229	609904.988432	46.035085
3442.168341	606927.817208	46.040090
3440.274445	603920.827333	46.045095
3437.970593	600853.678313	46.050100
3435.753455	597759.338377	46.055105
3433.693666	594620.805901	46.060109
3430.954252	591447.184800	46.065114
3428.610346	588233.856116	46.070119
3426.686398	584983.205802	46.075124
3424.044499	581714.507256	46.080129
3421.759418	578384.778423	46.085133
3419.097449	575039.528505	46.090138
3416.358804	571660.288351	46.095143
3414.362278	568246.050537	46.100148
3411.526527	564801.338063	46.105153
3409.133548	561311.422270	46.110157
3406.549461	557800.461962	46.115162
3403.727373	554264.529537	46.120167
3401.130367	550691.343750	46.125172
3398.135673	547093.543225	46.130177
3395.684080	543459.216451	46.135181
3393.006411	539803.404870	46.140186
3389.972688	536102.665398	46.145191
3387.031748	532393.944970	46.150196
3384.014710	528645.880857	46.155201
3381.451265	524886.948073	46.160205
3378.722626	521093.567902	46.165210
3375.707498	517263.071444	46.170215
3373.065608	513404.533386	46.175220
3369.851385	509536.147409	46.180225
3367.109031	505634.999980	46.185229
3363.686893	501722.257713	46.190234
3360.713720	497774.931090	46.195239
3357.724932	493792.177574	46.200244
3354.222965	489815.715886	46.205249
3350.938143	485806.474105	46.210253
3348.133115	481784.298694	46.215258
3344.538724	477736.849306	46.220263
3341.623391	473666.872248	46.225268
3338.062760	469593.281198	46.230273
3335.201931	465479.844034	46.235277
3331.906122	461375.595084	46.240282
3328.183582	457223.125088	46.245287
3325.419585	453073.553160	46.250292
3321.625303	448902.480769	46.255297
3318.282494	444725.899586	46.260301
3314.653435	440529.285753	46.265306
3311.102742	436323.393827	46.270311
3307.876710	432103.680272	46.275316
3303.944630	427865.555249	46.280321
3300.770894	423619.802895	46.285325
3297.081416	419367.232503	46.290330
3293.559496	415094.188096	46.295335
3290.194797	410816.146799	46.300340
3286.418451	406537.994785	46.305345
3282.937253	402245.383576	46.310349
3279.038511	397941.619737	46.315354
3275.406615	393624.572422	46.320359
3271.650057	389302.453220	46.325364
3268.039275	384980.446277	46.330369
3263.916750	380659.519062	46.335373
3260.585838	376321.857685	46.340378
3256.651813	371987.133030	46.345383
3253.077871	367634.226916	46.350388
3249.058199	363295.638213	46.355393
3245.705252	358944.423689	46.360397
3241.773136	354586.528882	46.365402
3237.701901	350234.976750	46.370407
3234.136372	345873.576898	46.375412
3230.098746	341512.839574	46.380417
3226.490497	337139.021554	46.385421
3222.307386	332767.474456	46.390426
3218.473196	328398.270688	46.395431
3214.832290	324031.813344	46.400436
3211.209953	319664.893845	46.405441
3207.163375	315282.101510	46.410445
3203.022315	310926.146427	46.415450
3198.861027	306555.488883	46.420455
3195.247117	302188.895495	46.425460
3191.160099	297832.233878	46.430465
3187.086091	293470.064921	46.435469
3183.142642	289128.821930	46.440474
3178.913667	284773.579833	46.445479
3175.298495	280424.124287	46.450484
3171.420376	276092.513670	46.455489
3167.107111	271747.981430	46.460493
3162.990409	267411.555810	46.465498
3158.936685	263094.128521	46.470503
3154.704095	258772.175901	46.475508
3150.348139	254466.235894	46.480513
3146.774668	250160.464757	46.485517
3142.551890	245869.838477	46.490522
3138.204521	241599.535638	46.495527
3134.204125	237313.817459	46.500532
3130.193607	233054.858751	46.505537
3126.023188	228789.697805	46.510541
3121.587459	224544.065419	46.515546
3117.543918	220309.747030	46.520551
3113.531886	216087.405071	46.525556
3109.034002	211874.188261	46.530561
3105.368289	207578.290310	46.535565
3100.853436	203372.211379	46.540570
3096.637172	199198.028460	46.545575
3092.786202	195020.792008	46.550580
3087.933200	190861.949216	46.555585
3084.002079	186725.269196	46.560589
3079.855954	182588.250361	46.565594
3075.704428	178472.786702	46.570599
3071.674597	174372.444148	46.575604
3067.279928	170282.787124	46.580609
3062.992709	166204.973055	46.585613
3058.690413	162143.881881	46.590618
3054.343198	158094.989857	46.595623
3050.171900	154059.824890	46.600628
3045.985989	150058.216349	46.605633
3041.592008	146049.947424	46.610637
3037.123644	142060.020778	46.615642
3032.660411	138090.339634	46.620647
3028.382194	134148.343675	46.625652
3023.632820	130231.274380	46.630657
3019.689077	126312.013720	46.635661
3015.254507	122432.871329	46.640666
3010.880652	118571.142909	46.645671
3006.448728	114714.585487	46.650676
3002.031876	110889.349003	46.655681
2997.629008	107091.879211	46.660685
2993.026647	103292.274731	46.665690
2988.691593	99543.245475	46.670695
2983.958688	95802.180695	46.675700
2979.042808	92103.383784	46.680705
2974.514768	88411.231261	46.685709
2969.638903	84752.687305	46.690714
2965.029069	81138.302938	46.695719
2960.064731	77544.625519	46.700724
2954.664990	74002.523380	46.705729
2949.690763	70481.050065	46.710733
2944.554632	66999.547142	46.715738
2938.608382	63578.836190	46.720743
2932.372110	60205.277348	46.725748
2923.649518	56963.872968	46.730753
2913.390254	53845.328307	46.735757
2902.748704	50850.828154	46.740762
2892.328502	47967.345915	46.745767
2882.784148	45219.005346	46.750772
2872.841405	42616.089469	46.755777
2864.253214	40153.122991	46.760781
2855.292021	37821.807505	46.765786
2846.972224	35612.613638	46.770791
2839.424707	33540.154847	46.775796
2831.255162	31598.896746	46.780801
2823.936643	29747.099696	46.785805
2816.616511	28024.080715	46.790810
2809.468123	26411.198052	46.795815
2802.902591	24910.346580	46.800820
2795.265816	23512.142703	46.805825
2788.569668	22218.106677	46.810829
2781.474899	21036.604101	46.815834
2774.543766	19939.249158	46.820839
2768.522148	18936.294913	46.825844
2761.752192	18021.578385	46.830849
2755.643560	17166.293455	46.835853
2750.143072	16400.620830	46.840858
2744.420814	15718.220354	46.845863
2739.118286	15069.784509	46.850868
2734.321549	14490.775526	46.855873
2729.925010	13955.574543	46.860877
2725.641659	13457.865023	46.865882
2721.773240	13008.974493	46.870887
2717.991608	12583.846041	46.875892
2714.227082	12191.393733	46.880897
2710.647229	11807.838827	46.885901
2707.361209	11447.531365	46.890906
2704.379146	11106.212129	46.895911
2701.406744	10763.795803	46.900916
2698.172036	10435.151664	46.905921
2695.035419	10105.133942	46.910925
2691.848175	9794.187021	46.915930
2689.049512	9473.765678	46.920935
2686.271398	9148.629000	46.925940
2683.139061	8840.355478	46.930945
2680.454628	8521.706562	46.935949
2677.547279	8203.062065	46.940954
2674.085904	7890.232315	46.945959
2670.948219	7568.844334	46.950964
2667.980654	7250.896076	46.955969
2665.070385	6915.686602	46.960973
2661.832436	6596.344556	46.965978
2658.471274	6269.727201	46.970983
2655.355541	5932.869826	46.975988
2652.115147	5610.222799	46.980993
2648.902761	5272.954785	46.985997
2645.674153	4936.288053	46.991002
2642.554549	4595.285166	46.996007
2639.054582	4264.132001	47.001012
2635.449983	3923.930342	47.006017
2632.524909	3589.730947	47.011021
2628.851751	3254.662192	47.016026
2625.267420	2911.558305	47.021031
2621.620428	2573.713652	47.026036
2617.771524	2244.413352	47.031041
2614.597993	1919.702215	47.036045
2610.627544	1587.767101	47.041050
2606.780083	1279.834006	47.046055
2603.362145	953.394928	47.051060
2598.814487	662.180479	47.056065
2595.011735	368.508876	47.061069
2589.819336	114.244026	47.066074
2574.392900	165.962531	47.071079
2564.711842	172.019418	47.076084
2558.853500	178.343318	47.081089
2556.261657	165.398361	47.086093
2555.006994	170.779926	47.091098
2553.564708	178.848462	47.096103
2552.047859	172.149312	47.101108
2549.357941	171.764473	47.106113
2546.617769	171.511070	47.111117
2543.366548	165.110408	47.116122
2539.714566	170.522759	47.121127
2536.403958	170.197743	47.126132
2532.462909	180.095595	47.131137
2529.292950	169.205460	47.136141
2526.449180	174.075539	47.141146
2522.926990	171.490585	47.146151
2519.892757	164.823437	47.151156
2516.280677	173.560713	47.156161
2512.883288	170.486485	47.161165
2510.013131	163.389493	47.166170
2506.183032	160.791633	47.171175
2502.968269	161.357401	47.176180
2499.429834	177.408385	47.181185
2496.237111	167.998729	47.186189
2493.204580	163.451737	47.191194
2489.561404	159.013826	47.196199
2485.724308	157.362791	47.201204
2482.581680	166.424383	47.206209
2479.326503	169.634087	47.211213
2476.349756	161.798504	47.216218
2472.592096	163.688261	47.221223
2469.364473	156.668653	47.226228
2465.480471	157.475942	47.231233
2462.183510	158.529708	47.236237
2458.571098	159.969839	47.241242
2454.155071	154.668879	47.246247
2451.958548	157.638536	47.251252
2448.472899	158.555914	47.256257
2444.950124	148.297959	47.261261
2441.161784	149.852391	47.266266
2437.609823	157.224061	47.271271
2434.415273	152.335028	47.276276
2431.224652	155.741507	47.281281
2427.944390	152.076516	47.286285
2424.484361	151.524041	47.291290
2420.829097	161.507397	47.296295
2417.542199	158.294625	47.301300
2413.961395	154.994602	47.306305
2410.181988	154.079259	47.311309
2407.201657	155.034222	47.316314
2403.127657	155.945149	47.321319
2400.275930	145.235853	47.326324
2395.960784	148.139464	47.331329
2393.161630	150.216597	47.336333
2389.860993	152.284552	47.341338
2386.163973	156.458040	47.346343
2382.800491	142.721586	47.351348
2379.288477	154.611297	47.356353
2375.972454	147.662004	47.361357
2372.346829	146.379514	47.366362
2368.614259	146.584859	47.371367
2365.439914	153.084356	47.376372
2361.766936	158.545480	47.381377
2358.192376	156.461067	47.386381
2355.065803	158.420388	47.391386
2351.476568	146.959449	47.396391
2348.244277	157.048063	47.401396
2344.412911	158.935282	47.406401
2341.089654	154.900333	47.411405
2337.606278	152.173738	47.416410
2333.556394	158.728399	47.421415
2330.362219	138.962553	47.426420
2327.179722	154.747839	47.431425
2323.947501	155.654251	47.436429
2320.035982	155.536727	47.441434
2316.474536	160.114137	47.446439
2313.341754	151.579603	47.451444
2309.750674	161.202156	47.456449
2306.447617	145.374052	47.461453
2302.875428	144.778019	47.466458
2299.134773	154.315942	47.471463
2295.860105	150.691956	47.476468
2292.099197	152.013651	47.481473
2288.609213	145.229309	47.486477
2284.966233	145.906565	47.491482
2281.660599	144.883702	47.496487
2278.367049	145.054721	47.501492
2275.094800	139.612071	47.506497
2271.451066	147.047737	47.511501
2268.033391	139.319640	47.516506
2264.661941	142.861256	47.521511
2260.922008	141.866893	47.526516
2257.284271	149.046420	47.531521
2253.634109	150.084832	47.536525
2250.791720	154.852205	47.541530
2246.674793	154.742013	47.546535
2243.419105	147.453696	47.551540
2239.885877	151.078874	47.556545
2235.981323	147.481966	47.561549
2233.251987	141.294541	47.566554
2229.548157	148.744303	47.571559
2226.064197	136.709404	47.576564
2222.592157	140.235291	47.581569
2219.102099	137.921144	47.586573
2215.807442	138.936013	47.591578
2211.915780	141.640009	47.596583
2208.115556	135.427342	47.601588
2205.021764	136.077918	47.606593
2201.684670	142.375859	47.611597
2198.310881	141.816805	47.616602
2194.724643	143.487044	47.621607
2190.925227	133.591321	47.626612
2187.343956	142.385273	47.631617
2183.741192	139.094976	47.636621
2180.738207	139.534419	47.641626
2176.910280	141.213398	47.646631
2173.778892	130.486905	47.651636
2170.525369	136.202136	47.656641
2166.720960	139.958967	47.661645
2163.263397	138.787812	47.666650
2159.547116	146.393600	47.671655
2155.854270	131.658532	47.676660
2152.243985	142.710118	47.681665
2149.004653	139.015481	47.686669
2145.792794	139.210398	47.691674
2142.205823	137.867234	47.696679
2138.791612	138.835589	47.701684
2135.183715	138.687813	47.706689
2131.915917	138.442044	47.711693
2128.014733	132.568569	47.716698
2124.556949	150.364505	47.721703
2121.390726	146.635513	47.726708
2117.625528	137.282016	47.731713
2114.131626	141.354861	47.736717
2110.545091	127.386903	47.741722
2106.947317	148.173739	47.746727
2103.572596	132.439156	47.751732
2100.335061	138.421552	47.756737
2097.070192	136.930708	47.761741
2093.161270	135.892748	47.766746
2089.492872	147.419297	47.771751
2086.208700	142.412898	47.776756
2082.730972	137.745130	47.781761
2079.165938	142.406764	47.786765
2075.894577	137.014829	47.791770
2072.605237	137.113856	47.796775
2069.112612	127.465367	47.801780
2064.860466	141.254316	47.806785
2061.311105	140.486756	47.811789
2058.029087	135.640461	47.816794
2054.742015	137.471562	47.821799
2051.456225	126.499914	47.826804
2047.729741	126.695422	47.831809
2044.008883	131.934372	47.836813
2040.496990	131.294832	47.841818
2037.251055	128.730143	47.846823
2033.774378	128.572021	47.851828
2030.241501	122.212744	47.856833
2026.777488	134.228122	47.861837
2023.380119	118.254046	47.866842
2019.457024	128.811923	47.871847
2016.581131	124.414433	47.876852
2012.762954	130.209001	47.881857
2009.161416	133.294646	47.886861
2005.785179	127.051601	47.891866
2001.983244	132.747193	47.896871
1998.889571	123.301060	47.901876
1995.248544	133.279164	47.906881
1991.799009	131.944398	47.911885
1988.068102	129.014447	47.916890
1984.508595	130.974063	47.921895
1981.366184	121.778324	47.926900
1977.654483	133.742680	47.931905
1974.224921	129.537104	47.936909
1970.714873	124.561195	47.941914
1967.024599	125.078761	47.946919
1964.101803	124.898279	47.951924
1960.498006	126.920678	47.956929
1956.823659	130.416615	47.961933
1953.455537	122.437273	47.966938
1949.539977	132.307022	47.971943
1946.078143	127.112411	47.976948
1942.735829	131.674005	47.981953
1939.553215	121.872597	47.986957
1935.767371	120.082118	47.991962
1931.980806	131.161372	47.996967
1928.713569	128.260265	48.001972
1925.146554	128.991943	48.006977
1921.673971	128.649504	48.011981
1918.600695	125.013055	48.016986
1914.806689	126.192499	48.021991
1911.289793	131.842458	48.026996
1907.754399	127.812285	48.032001
1904.482368	135.936092	48.037005
1901.097881	127.136986	48.042010
1897.384543	130.850164	48.047015
1893.599708	121.405001	48.052020
1890.312923	122.287164	48.057025
1886.152269	130.430870	48.062029
1883.498017	121.881567	48.067034
1879.708411	131.476981	48.072039
1876.393580	131.145617	48.077044
1872.519939	131.058905	48.082049
1869.458755	124.537185	48.087053
1865.983852	121.080977	48.092058
1862.090278	122.532265	48.097063
1858.982151	117.925186	48.102068
1855.356429	129.140529	48.107073
1851.381946	127.829432	48.112077
1848.142392	131.132857	48.117082
1844.781207	125.874536	48.122087
1841.478918	127.772821	48.127092
1837.682693	123.844399	48.132097
1834.121726	111.747193	48.137101
1830.282956	116.022040	48.142106
1826.730321	120.348097	48.147111
1823.740522	119.065191	48.152116
1820.118016	116.617725	48.157121
1817.000678	126.652700	48.162125
1813.606698	117.867670	48.167130
1809.589053	130.183612	48.172135
1806.516033	127.928366	48.177140
1802.779718	123.686768	48.182145
1799.255861	116.448826	48.187149
1795.912151	121.152433	48.192154
1791.602655	129.415721	48.197159
1789.025619	128.899783	48.202164
1785.382281	116.358202	48.207169
1781.672744	122.622809	48.212173
1778.587909	122.018687	48.217178
1774.778996	120.999400	48.222183
1771.322875	110.244390	48.227188
1767.670578	126.839460	48.232193
1763.984773	125.137775	48.237197
1760.701002	119.622427	48.242202
1757.119374	123.863140	48.247207
1754.048357	108.819324	48.252212
1750.381571	122.720965	48.257217
1746.633315	120.143170	48.262221
1743.116330	123.307984	48.267226
1739.701861	125.973966	48.272231
1736.016886	109.090186	48.277236
1732.569845	115.920048	48.282241
1729.184849	123.023832	48.287245
1725.849398	114.957974	48.292250
1722.057558	121.536767	48.297255
1718.552228	115.522284	48.302260
1715.283733	120.563002	48.307265
1711.615259	118.886124	48.312269
1708.404884	111.518322	48.317274
1704.620664	117.462215	48.322279
1701.320512	105.364468	48.327284
1697.609983	116.829536	48.332289
1694.283809	116.531750	48.337293
1690.923197	114.879802	48.342298
1686.957230	128.251534	48.347303
1683.752550	114.023546	48.352308
1680.460751	112.059100	48.357313
1676.555583	114.851585	48.362317
1673.123197	116.740300	48.367322
1669.398177	127.728258	48.372327
1666.245965	121.751379	48.377332
1662.614528	121.570357	48.382337
1658.981158	124.065555	48.387341
1655.906171	117.612182	48.392346
1652.331793	125.899561	48.397351
1648.597546	122.932553	48.402356
1645.073855	116.190422	48.407361
1641.602183	126.023555	48.412365
1638.148877	125.339509	48.417370
1634.487446	126.956868	48.422375
1631.123146	118.241085	48.427380
1627.864069	127.752960	48.432385
1623.661194	123.179128	48.437389
1621.107777	117.037630	48.442394
1617.201424	125.894937	48.447399
1613.744438	114.766246	48.452404
1609.848070	117.963452	48.457409
1606.580011	124.495843	48.462413
1603.276979	124.746053	48.467418
1599.477185	128.686468	48.472423
1596.201910	117.742665	48.477428
1592.473738	115.058078	48.482433
1589.066345	123.716725	48.487437
1585.943218	113.263633	48.492442
1582.013268	118.322763	48.497447
1578.592497	118.739264	48.502452
1574.951127	108.060816	48.507457
1571.613598	116.648330	48.512461
1568.053833	105.306771	48.517466
1564.612050	116.565111	48.522471
1561.285040	110.186016	48.527476
1557.495634	113.783351	48.532481
1554.009872	113.860337	48.537485
1550.920865	112.898692	48.542490
1547.088238	117.649905	48.547495
1543.345643	116.115653	48.552500
1540.090924	110.132920	48.557505
1536.255615	117.724267	48.562509
1533.346095	112.352875	48.567514
1529.764093	115.264350	48.572519
1526.043738	120.052281	48.577524
1522.210116	103.707146	48.582529
1518.758619	116.782028	48.587533
1515.598484	111.357737	48.592538
1511.908262	114.393474	48.597543
1508.379982	113.562862	48.602548
1505.097011	109.412957	48.607553
1501.547346	114.522970	48.612557
1498.396953	102.084118	48.617562
1494.689138	119.299278	48.622567
1491.094765	99.747179	48.627572
1487.606737	107.816739	48.632577
1484.050336	113.504891	48.637581
1480.606645	112.916070	48.642586
1477.002291	113.182028	48.647591
1473.567005	105.297851	48.652596
1469.807088	112.989268	48.657601
1466.069847	110.924937	48.662605
1462.953950	109.496160	48.667610
1459.368955	115.112095	48.672615
1456.065562	99.730812	48.677620
1452.462698	111.528916	48.682625
1448.725343	111.551063	48.687629
1445.551389	116.806227	48.692634
1442.172746	119.756779	48.697639
1438.458319	121.760751	48.702644
1434.939272	112.260046	48.707649
1431.397184	120.784763	48.712653
1428.244371	111.056588	48.717658
1424.360760	114.752281	48.722663
1421.051149	109.285868	48.727668
1417.659813	117.026522	48.732673
1413.892243	115.535972	48.737677
1410.751159	117.247868	48.742682
1406.743038	127.004249	48.747687
1403.387327	117.083279	48.752692
1399.891391	118.530594	48.757697
1396.310246	117.074959	48.762701
1393.040547	113.021415	48.767706
1389.733086	124.654315	48.772711
1386.316232	116.165477	48.777716
1382.184279	119.319713	48.782721
1379.034026	128.034073	48.787725
1375.516934	115.404906	48.792730
1371.495927	122.693770	48.797735
1368.151734	112.340143	48.802740
1365.144943	118.894621	48.807745
1361.611805	111.673973	48.812749
1358.167618	112.733878	48.817754
1354.232714	113.135673	48.822759
1350.867345	102.757939	48.827764
1347.707543	120.737473	48.832769
1343.789201	119.089365	48.837773
1340.330020	115.298065	48.842778
1336.967833	122.628033	48.847783
1333.358997	116.262153	48.852788
1329.976165	118.615150	48.857793
1326.449668	111.156038	48.862797
1322.966183	118.140004	48.867802
1319.157620	115.062420	48.872807
1315.642297	109.422692	48.877812
1312.498367	119.902600	48.882817
1308.776099	105.583680	48.887821
1305.546954	118.947347	48.892826
1302.021459	118.345543	48.897831
1298.753888	114.720136	48.902836
1294.877179	116.547592	48.907841
1291.453190	112.281641	48.912845
1287.822886	111.192978	48.917850
1284.211948	112.251297	48.922855
1280.558482	107.056341	48.927860
1277.026305	114.669602	48.932865
1274.047374	117.208660	48.937869
1270.906291	109.757122	48.942874
1266.987201	117.262076	48.947879
1263.506062	111.583192	48.952884
1259.773871	114.412741	48.957889
1256.129688	110.793384	48.962893
1252.664082	107.561680	48.967898
1249.343653	111.872259	48.972903
1245.884943	113.273475	48.977908
1242.252572	109.963377	48.982913
1238.400536	119.056881	48.987917
1235.370916	109.126945	48.992922
1231.955707	117.497421	48.997927
1228.574784	104.582244	49.002932
1225.027139	115.069148	49.007937
1221.252968	108.408647	49.012941
1218.127031	100.732054	49.017946
1214.273846	111.067796	49.022951
1210.627772	107.701777	49.027956
1207.216749	111.653211	49.032961
1204.121652	110.620387	49.037965
1200.517689	104.801429	49.042970
1196.665968	114.782134	49.047975
1193.175596	103.463973	49.052980
1189.625128	115.031784	49.057985
1186.066017	111.337839	49.062989
1183.019624	100.350434	49.067994
1179.246076	113.475608	49.072999
1176.095322	99.330121	49.078004
1172.280464	103.626786	49.083009
1168.594341	115.610133	49.088013
1165.129197	111.205453	49.093018
1161.402815	118.080700	49.098023
1158.339714	111.986660	49.103028
1154.770960	104.555996	49.108033
1151.140076	116.039644	49.113037
1148.256643	104.255905	49.118042
1144.373733	100.980013	49.123047
1140.638934	107.762140	49.128052
1137.119073	106.377686	49.133057
1133.701801	98.136403	49.138061
1130.118163	105.569025	49.143066
1126.771841	111.092456	49.148071
1123.424265	97.470926	49.153076
1119.712976	104.264374	49.158081
1115.926788	105.776863	49.163085
1112.690510	96.405918	49.168090
1109.235043	100.453372	49.173095
1105.636046	99.272064	49.178100
1102.277120	99.354272	49.183105
1098.682117	98.201910	49.188109
1095.583598	93.644911	49.193114
1091.889230	104.294885	49.198119
1088.183682	101.620008	49.203124
1084.459506	104.303129	49.208129
1080.996420	103.048060	49.213133
1077.634202	95.083268	49.218138
1074.030334	100.166041	49.223143
1070.868497	102.759346	49.228148
1067.309438	98.897956	49.233153
1063.803795	107.185613	49.238157
1060.316297	105.682796	49.243162
1056.447218	111.127743	49.248167
1053.108702	106.768127	49.253172
1049.529475	109.821191	49.258177
1045.813235	104.604061	49.263181
1042.569564	103.076332	49.268186
1039.046030	107.235340	49.273191
1035.653890	101.305129	49.278196
1032.124384	100.340313	49.283201
1028.554008	108.381966	49.288205
1025.251482	109.340352	49.293210
1021.668488	117.428896	49.298215
1018.175627	102.173856	49.303220
1014.699154	104.771079	49.308225
1011.093613	112.643129	49.313229
1007.634893	105.101452	49.318234
1004.063929	110.283230	49.323239
1000.488050	107.921666	49.328244
997.303272	104.289706	49.333249
993.693165	113.351672	49.338253
990.128051	109.133574	49.343258
986.532614	111.932238	49.348263
983.293522	105.035466	49.353268
979.628683	110.233181	49.358273
975.638554	110.125836	49.363277
972.888276	96.019083	49.368282
968.755874	118.315343	49.373287
965.628913	104.087556	49.378292
962.383374	109.549440	49.383297
958.452694	107.656650	49.388301
955.075442	101.435538	49.393306
951.330703	115.993108	49.398311
948.033319	97.056675	49.403316
944.831519	105.075122	49.408321
941.019527	103.978901	49.413325
937.696773	115.101720	49.418330
934.198314	109.572991	49.423335
930.430756	112.160994	49.428340
926.760527	105.992501	49.433345
923.171336	107.067241	49.438349
920.033904	99.657015	49.443354
916.264537	105.928600	49.448359
912.912743	98.491671	49.453364
909.620394	100.158275	49.458369
906.084276	117.529718	49.463373
902.935774	99.256614	49.468378
899.637583	104.115702	49.473383
895.830574	108.674538	49.478388
892.011667	107.784337	49.483393
888.306618	109.992820	49.488397
885.013681	109.393532	49.493402
881.347620	101.077773	49.498407
877.852073	107.285354	49.503412
874.586614	102.594706	49.508417
870.538059	101.510835	49.513421
867.139512	107.642193	49.518426
863.659632	109.803586	49.523431
860.725741	111.367524	49.528436
857.326662	104.464951	49.533441
853.233174	113.154279	49.538445
850.057808	102.192417	49.543450
846.602098	116.721790	49.548455
843.079607	106.053951	49.553460
839.885511	110.748455	49.558465
835.657279	101.591930	49.563469
832.470289	99.577233	49.568474
828.787804	108.181823	49.573479
825.512446	105.913172	49.578484
821.823357	102.757262	49.583489
818.399196	97.449202	49.588493
814.998298	95.832406	49.593498
811.392254	97.659700	49.598503
808.206154	99.940079	49.603508
804.706847	102.338178	49.608513
800.695398	103.804124	49.613517
797.376257	104.000750	49.618522
793.637894	109.968537	49.623527
790.519033	93.019498	49.628532
787.199621	96.486813	49.633537
783.381920	103.775275	49.638541
780.094489	93.970246	49.643546
776.072907	99.931810	49.648551
772.774475	95.131652	49.653556
769.589480	97.767473	49.658561
765.813563	97.038007	49.663565
762.782980	87.150056	49.668570
759.188318	97.108092	49.673575
755.521357	110.515090	49.678580
751.995322	100.619901	49.683585
748.270498	99.735575	49.688589
744.562934	91.590009	49.693594
741.074526	100.098224	49.698599
737.887170	95.475673	49.703604
734.396709	89.007272	49.708609
730.918427	98.359991	49.713613
727.191889	87.602297	49.718618
723.536923	102.457937	49.723623
720.181806	94.905293	49.728628
716.945928	96.372068	49.733633
713.245904	104.437761	49.738637
710.362772	94.987020	49.743642
706.650901	100.043142	49.748647
702.957221	100.751329	49.753652
699.236614	94.904945	49.758657
695.525139	100.041128	49.763661
692.529695	95.379563	49.768666
688.797148	102.349325	49.773671
685.611699	100.776710	49.778676
681.964883	98.829318	49.783681
678.091177	105.618004	49.788685
674.915899	94.865652	49.793690
671.346048	101.880144	49.798695
667.822253	94.062606	49.803700
664.077938	97.857039	49.808705
660.749902	102.320048	49.813709
657.240284	102.851004	49.818714
653.891606	103.033088	49.823719
650.393820	93.543188	49.828724
646.793869	92.733011	49.833729
642.733563	101.098125	49.838733
639.900743	92.223030	49.843738
636.311250	101.388001	49.848743
632.523899	104.242965	49.853748
629.340517	98.698087	49.858753
625.866082	103.472268	49.863757
622.415941	90.299934	49.868762
618.510231	100.618366	49.873767
615.111076	100.665763	49.878772
611.704097	92.470982	49.883777
608.125183	102.998992	49.888781
604.936340	95.505762	49.893786
601.077276	90.883161	49.898791
597.334161	98.725186	49.903796
594.412937	98.296484	49.908801
590.864831	103.557668	49.913805
587.726769	92.691488	49.918810
583.698638	101.997747	49.923815
579.897181	96.391981	49.928820
576.635777	98.982168	49.933825
573.038512	106.356671	49.938829
569.849392	98.820889	49.943834
565.912590	101.309322	49.948839
563.059697	95.905767	49.953844
559.336751	96.225234	49.958849
555.733673	95.324481	49.963853
552.601247	96.114567	49.968858
548.507829	97.416306	49.973863
544.730034	103.278726	49.978868
541.533903	100.106810	49.983873
538.280626	97.886035	49.988877
534.840918	88.858065	49.993882
531.324629	93.583197	49.998887
527.565249	96.304759	50.003892
524.176488	96.286374	50.008897
520.358846	87.386077	50.013901
517.287076	94.652742	50.018906
513.614734	94.928551	50.023911
509.967161	92.078033	50.028916
506.855932	91.966178	50.033921
503.136839	97.571457	50.038925
499.820413	98.413143	50.043930
496.087432	96.136017	50.048935
492.299915	90.429558	50.053940
489.486770	90.719100	50.058945
485.526173	96.150447	50.063949
482.270378	86.369451	50.068954
478.443416	99.083430	50.073959
475.211702	92.581116	50.078964
471.801434	92.588629	50.083969
468.571370	105.717109	50.088973
464.577932	92.764873	50.093978
460.890136	94.771738	50.098983
457.557205	96.386780	50.103988
453.922637	96.448003	50.108993
450.304661	95.506785	50.113997
447.133917	94.315139	50.119002
443.630541	96.432002	50.124007
439.995432	83.825232	50.129012
436.519768	89.493285	50.134017
432.899390	98.832826	50.139021
429.448662	90.154082	50.144026
425.981217	95.219703	50.149031
422.315175	96.422217	50.154036
419.379960	88.530583	50.159041
415.716540	93.018092	50.164045
412.391933	90.550318	50.169050
408.374892	94.684126	50.174055
405.170512	94.711884	50.179060
401.619792	98.288800	50.184065
397.858234	102.028882	50.189069
394.582355	89.012233	50.194074
391.071250	101.259008	50.199079
387.471520	98.849811	50.204084
384.036548	103.220604	50.209089
380.482529	98.211265	50.214093
377.020819	94.160301	50.219098
373.392102	101.380908	50.224103
370.220032	94.901565	50.229108
366.532996	90.337342	50.234113
363.164396	95.301796	50.239117
359.463020	93.165785	50.244122
355.871972	98.134306	50.249127
352.325083	93.929136	50.254132
348.998950	90.670748	50.259137
345.539074	103.050763	50.264141
341.940952	90.209054	50.269146
338.373334	91.922427	50.274151
334.941011	92.327579	50.279156
331.327581	92.776128	50.284161
328.152582	95.435468	50.289165
324.990360	92.268173	50.294170
320.819328	90.853837	50.299175
317.529646	96.983941	50.304180
313.999161	93.610813	50.309185
310.546589	99.832808	50.314189
307.301236	95.901590	50.319194
303.562324	89.742669	50.324199
299.865376	90.528500	50.329204
296.261716	87.695963	50.334209
292.335027	89.609509	50.339213
289.242723	82.947918	50.344218
285.647757	85.680947	50.349223
282.666316	96.659665	50.354228
279.381832	84.983263	50.359233
275.157590	100.442365	50.364237
272.016275	87.718892	50.369242
268.555399	89.087275	50.374247
265.013736	88.184890	50.379252
261.649479	93.110614	50.384257
257.538056	91.543603	50.389261
254.177730	86.576119	50.394266
250.778636	89.741673	50.399271
246.969874	83.797033	50.404276
244.065103	82.001478	50.409281
240.117147	91.723157	50.414285
237.363424	83.413071	50.419290
233.437466	91.868768	50.424295
230.081565	90.352538	50.429300
226.417474	93.024836	50.434305
222.991469	92.379212	50.439309
219.544347	88.486600	50.444314
215.926181	87.810436	50.449319
212.280767	86.634006	50.454324
208.732107	88.346714	50.459329
205.096428	87.047121	50.464333
201.882262	80.158712	50.469338
198.103521	89.071757	50.474343
194.904451	87.974384	50.479348
191.202579	90.989617	50.484353
187.625128	88.539808	50.489357
184.374278	82.089055	50.494362
181.228383	91.955451	50.499367
177.623638	90.724562	50.504372
174.215786	89.802074	50.509377
170.087893	95.279545	50.514381
166.683557	78.705921	50.519386
162.739897	89.105582	50.524391
159.661788	87.522304	50.529396
156.470042	83.137545	50.534401
152.831272	87.091933	50.539405
149.355594	81.618729	50.544410
145.802021	88.925930	50.549415
142.020488	84.929304	50.554420
138.997265	83.080421	50.559425
135.235546	83.502380	50.564429
131.739194	77.128826	50.569434
128.355661	84.391704	50.574439
124.892522	86.735208	50.579444
121.551179	82.068984	50.584449
117.799150	92.368481	50.589453
114.499324	81.271380	50.594458
110.869268	86.969383	50.599463
107.556895	86.456593	50.604468
103.699522	84.865036	50.609473
100.028753	88.032668	50.614477
96.529641	85.981803	50.619482
93.118978	95.459539	50.624487
89.722017	82.042504	50.629492
86.457146	89.447186	50.634497
82.351101	98.766763	50.639501
79.267678	90.664314	50.644506
75.784588	88.318562	50.649511
72.032042	90.704700	50.654516
68.594821	86.517734	50.659521
65.006430	96.088658	50.664525
61.961500	96.611035	50.669530
58.168958	103.818955	50.674535
54.838122	95.772290	50.679540
51.425093	96.042260	50.684545
47.386568	82.950538	50.689549
44.314470	86.774873	50.694554
40.587346	84.929940	50.699559
37.216091	87.205611	50.704564
33.836031	91.102656	50.709569
30.120502	101.435058	50.714573
26.987700	79.171873	50.719578
23.259452	80.569334	50.724583
19.520117	90.262174	50.729588
16.037360	87.996930	50.734593
12.361842	97.082080	50.739597
9.190439	84.288639	50.744602
5.948587	89.514751	50.749607
1.928988	80.385171	50.754612