Tue Jun 21 11:19:11 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.558084	83.568177	0.000000
0.885573	88.842174	0.005005
0.869039	80.715223	0.010010
0.732469	79.119945	0.015014
1.018747	78.805387	0.020019
0.781075	72.938412	0.025024
0.394973	56.901217	0.030029
0.384080	44.697641	0.035034
-0.243386	45.600787	0.040038
-0.289221	32.684125	0.045043
-0.984213	24.758556	0.050048
-1.114947	25.500508	0.055053
-1.317120	15.994591	0.060058
-2.174947	20.051760	0.065062
-2.688061	28.155963	0.070067
-3.294806	25.145734	0.075072
-3.088689	28.108723	0.080077
-3.073477	20.746932	0.085082
-3.432415	22.329817	0.090086
-3.079952	25.841820	0.095091
-3.499322	25.731934	0.100096
-3.386859	20.807470	0.105101
-4.249708	28.656424	0.110106
-4.377282	31.322435	0.115110
-4.764807	21.929499	0.120115
-5.104100	36.868730	0.125120
-5.364753	18.886611	0.130125
-5.640550	24.810062	0.135130
-6.105708	30.849727	0.140134
-6.193756	23.450769	0.145139
-6.854210	30.937846	0.150144
-6.617912	26.489954	0.155149
-6.466001	21.513769	0.160154
-6.941262	24.661425	0.165158
-6.749990	24.879611	0.170163
-7.381696	29.370961	0.175168
-7.844287	21.308834	0.180173
-8.020344	30.051236	0.185178
-8.240430	32.688563	0.190182
-7.938269	28.406376	0.195187
-9.004053	32.707160	0.200192
-9.337113	23.204367	0.205197
-9.770154	31.376217	0.210202
-9.673292	24.534095	0.215206
-9.911769	21.188984	0.220211
-10.031728	23.181225	0.225216
-9.785416	21.437693	0.230221
-10.178091	23.699267	0.235226
-10.971612	26.518580	0.240230
-10.779508	26.428593	0.245235
-11.094024	19.812071	0.250240
-11.049426	15.190505	0.255245
-11.969881	20.322063	0.260250
-12.528906	25.219325	0.265254
-12.658290	22.014211	0.270259
-12.963803	22.839374	0.275264
-12.823836	20.942367	0.280269
-12.926828	18.627192	0.285274
-12.850702	23.720793	0.290278
-12.876904	18.747466	0.295283
-13.710644	26.957453	0.300288
-13.978618	15.937649	0.305293
-14.280632	27.433368	0.310298
-14.600689	26.348001	0.315302
-15.100232	23.845912	0.320307
-15.728077	24.451347	0.325312
-15.279161	18.147067	0.330317
-15.581884	24.014198	0.335322
-15.996470	27.560680	0.340326
-15.866456	23.175184	0.345331
-16.260489	27.197976	0.350336
-16.048479	24.720721	0.355341
-16.946668	16.595169	0.360346
-17.429869	26.069032	0.365350
-17.152114	26.167323	0.370355
-17.873697	20.953760	0.375360
-17.714913	25.668608	0.380365
-17.828264	31.069855	0.385370
-17.782350	33.712464	0.390374
-18.787710	26.392209	0.395379
-19.465392	25.886432	0.400384
-19.075789	23.531514	0.405389
-19.211273	25.106009	0.410394
-19.157152	25.851289	0.415398
-19.392747	16.243956	0.420403
-20.308748	23.317908	0.425408
-20.244677	25.913109	0.430413
-20.692878	19.413842	0.435418
-20.848171	24.178335	0.440422
-20.681016	20.995941	0.445427
-21.389959	20.284394	0.450432
-22.098719	16.746626	0.455437
-22.296372	16.078671	0.460442
-22.458998	18.225779	0.465446
-22.421016	21.707966	0.470451
-22.763175	24.436154	0.475456
-22.698804	16.037335	0.480461
-22.536103	24.390931	0.485466
-22.768766	22.162350	0.490470
-23.241201	23.012198	0.495475
-23.594460	23.081593	0.500480
-23.775945	29.534261	0.505485
-24.088729	33.743300	0.510490
-25.020159	26.870982	0.515494
-25.085978	26.682813	0.520499
-25.346232	23.793003	0.525504
-25.507632	20.573065	0.530509
-25.652449	25.439817	0.535514
-25.757283	31.035604	0.540518
-25.867664	24.281084	0.545523
-26.311432	27.694267	0.550528
-26.504132	24.958041	0.555533
-27.048233	28.391392	0.560538
-27.558842	25.787932	0.565542
-27.388386	16.954779	0.570547
-27.586162	29.576381	0.575552
-27.475564	22.983388	0.580557
-27.793532	19.090033	0.585562
-28.314918	32.818985	0.590566
-28.611017	24.852225	0.595571
-28.950586	31.019289	0.600576
-28.607009	23.964828	0.605581
-29.290625	32.828584	0.610586
-30.358548	30.674987	0.615590
-29.907892	18.802687	0.620595
-30.599581	26.813920	0.625600
-30.152096	22.937259	0.630605
-30.380519	18.451681	0.635610
-30.460477	25.639567	0.640614
-30.670145	20.520011	0.645619
-31.604146	31.009415	0.650624
-31.943587	17.832372	0.655629
-32.288672	15.762517	0.660634
-32.282199	14.294912	0.665638
-32.048538	19.536468	0.670643
-32.427421	22.055842	0.675648
-32.258183	14.422475	0.680653
-33.106323	20.645147	0.685658
-33.228036	24.681448	0.690662
-33.666063	22.298821	0.695667
-33.969252	27.004928	0.700672
-33.566680	17.721699	0.705677
-34.030069	18.962543	0.710682
-34.674176	23.877646	0.715686
-34.965034	14.374584	0.720691
-35.385472	26.220641	0.725696
-35.239441	24.047943	0.730701
-35.424542	23.545445	0.735706
-35.911156	38.269314	0.740710
-36.131206	17.916241	0.745715
-36.609725	28.680278	0.750720
-36.562652	22.215219	0.755725
-36.660197	23.164991	0.760730
-36.538086	30.092876	0.765734
-37.231193	25.605123	0.770739
-37.719839	30.962358	0.775744
-38.032509	18.753138	0.780749
-38.304803	22.002552	0.785754
-38.190124	26.459489	0.790758
-38.296441	15.794755	0.795763
-39.167268	28.338381	0.800768
-39.511766	23.806118	0.805773
-39.546891	32.040334	0.810778
-39.726108	29.015547	0.815782
-39.391596	24.805357	0.820787
-39.877137	25.467148	0.825792
-39.962846	27.005575	0.830797
-40.892030	28.359674	0.835802
-40.997126	29.259588	0.840806
-41.095626	24.315204	0.845811
-41.256242	28.232643	0.850816
-41.445338	27.725282	0.855821
-42.191103	31.530260	0.860826
-42.604024	27.543506	0.865830
-42.790389	12.684317	0.870835
-43.068303	18.712899	0.875840
-42.750983	22.979790	0.880845
-43.235814	25.134874	0.885850
-43.209484	14.015424	0.890854
-43.155845	11.330757	0.895859
-43.562866	24.271363	0.900864
-43.805207	22.062739	0.905869
-44.472193	24.981672	0.910874
-44.635072	24.987768	0.915878
-44.420947	25.319383	0.920883
-45.332555	31.051348	0.925888
-46.197631	25.357962	0.930893
-45.690962	23.064561	0.935898
-45.715853	28.246522	0.940902
-46.189698	32.928009	0.945907
-46.528316	29.406099	0.950912
-46.406463	28.091458	0.955917
-46.671908	22.261668	0.960922
-47.033398	31.045435	0.965926
-47.330887	21.724619	0.970931
-47.551469	28.702745	0.975936
-47.861159	17.115224	0.980941
-47.858799	23.155406	0.985946
-48.272644	31.126942	0.990950
-48.838513	22.628457	0.995955
-49.368403	30.501207	1.000960
-49.480393	15.672915	1.005965
-49.418750	19.055871	1.010970
-49.538703	29.702312	1.015974
-48.976976	21.559548	1.020979
-49.955914	29.725705	1.025984
-50.605346	16.940404	1.030989
-50.896444	23.487195	1.035994
-51.329069	27.996293	1.040998
-51.252914	21.203583	1.046003
-51.164554	34.233043	1.051008
-50.996790	20.823410	1.056013
-52.019701	26.668921	1.061018
-52.362578	36.961766	1.066022
-52.507663	23.111402	1.071027
-52.670381	33.741841	1.076032
-52.689608	25.234913	1.081037
-52.507802	30.777110	1.086042
-53.451347	24.941224	1.091046
-53.623081	23.372301	1.096051
-54.008345	29.246987	1.101056
-54.089463	18.093433	1.106061
-54.486491	29.979818	1.111066
-54.947549	22.986592	1.116070
-55.321218	28.539088	1.121075
-55.606457	28.456522	1.126080
-55.513632	24.819747	1.131085
-55.823636	27.139659	1.136090
-56.088428	33.434643	1.141094
-55.983312	23.625253	1.146099
-55.997520	21.244267	1.151104
-55.866751	10.243289	1.156109
-57.106470	25.356494	1.161114
-57.501333	27.589821	1.166118
-57.725302	18.328069	1.171123
-57.878941	29.258918	1.176128
-57.439274	16.046188	1.181133
-57.553974	21.933288	1.186138
-58.692632	23.144877	1.191142
-58.652529	19.569918	1.196147
-59.517480	22.731402	1.201152
-59.421792	15.710501	1.206157
-59.351952	21.355103	1.211162
-59.676805	23.516846	1.216166
-59.587034	21.310841	1.221171
-60.035409	24.813192	1.226176
-60.364798	20.122143	1.231181
-60.449011	16.536200	1.236186
-61.012837	17.776118	1.241190
-60.802595	17.573210	1.246195
-61.641608	23.593688	1.251200
-61.817296	23.557902	1.256205
-61.826050	18.341534	1.261210
-61.941758	26.080765	1.266214
-62.087823	21.709618	1.271219
-62.454538	29.839107	1.276224
-63.105707	21.994110	1.281229
-63.516151	23.910733	1.286234
-63.661936	28.375483	1.291238
-63.697733	29.014492	1.296243
-63.657566	25.340657	1.301248
-63.648852	23.349356	1.306253
-64.371698	21.950048	1.311258
-64.955474	21.830495	1.316262
-64.964423	17.867220	1.321267
-65.421695	28.487237	1.326272
-65.532324	23.107774	1.331277
-65.276489	15.751525	1.336282
-65.767200	26.915007	1.341286
-66.196244	17.116340	1.346291
-66.824259	19.544567	1.351296
-66.707635	13.999598	1.356301
-66.624760	13.617690	1.361306
-66.895746	23.894278	1.366310
-67.031049	19.504774	1.371315
-68.148569	35.397341	1.376320
-68.390121	19.916222	1.381325
-68.186401	21.600100	1.386330
-68.598791	24.569221	1.391334
-68.232251	15.803051	1.396339
-68.565808	27.666490	1.401344
-69.098134	22.083564	1.406349
-69.851326	20.725987	1.411354
-69.903665	19.933131	1.416358
-69.986175	11.859379	1.421363
-70.311463	25.884601	1.426368
-70.412551	23.292848	1.431373
-70.395212	22.599748	1.436378
-71.051780	22.022798	1.441382
-71.441886	16.140252	1.446387
-71.909041	20.052021	1.451392
-71.752328	19.525671	1.456397
-71.601394	21.050953	1.461402
-72.042528	35.020186	1.466406
-71.819879	18.553078	1.471411
-73.156801	18.945428	1.476416
-73.123843	12.463571	1.481421
-73.400430	20.706591	1.486426
-73.653232	23.240804	1.491430
-73.475335	17.432904	1.496435
-74.008166	16.788891	1.501440
-73.659514	14.675184	1.506445
-74.063814	21.688864	1.511450
-75.086296	16.561460	1.516454
-74.918957	14.295249	1.521459
-75.204260	18.829871	1.526464
-75.156095	14.207323	1.531469
-75.817581	12.172511	1.536474
-76.360680	13.051629	1.541478
-76.364113	8.713894	1.546483
-76.417541	15.640057	1.551488
-76.550429	22.607996	1.556493
-76.669573	10.667670	1.561498
-77.138388	14.562150	1.566502
-77.553236	9.156711	1.571507
-78.412067	16.281188	1.576512
-78.379059	12.595124	1.581517
-78.436177	16.494037	1.586522
-78.478689	9.116164	1.591526
-78.553125	16.907753	1.596531
-78.604562	10.603266	1.601536
-78.834275	12.323803	1.606541
-79.591166	16.637374	1.611546
-80.043544	11.921510	1.616550
-80.207655	13.527780	1.621555
-80.112908	11.108426	1.626560
-80.191655	21.284107	1.631565
-80.009433	13.381009	1.636570
-81.033065	13.880918	1.641574
-81.326525	9.083087	1.646579
-81.489294	17.277656	1.651584
-81.512223	16.621219	1.656589
-81.718171	14.263901	1.661594
-82.307055	14.631817	1.666598
-82.946023	1.187098	1.671603
-83.676955	9.291849	1.676608
-83.128815	8.794600	1.681613
-83.462625	13.424278	1.686618
-83.776279	11.776250	1.691622
-83.249108	13.362155	1.696627
-83.750050	17.121654	1.701632
-83.585160	14.084281	1.706637
-84.394357	7.341718	1.711642
-84.798297	15.124338	1.716646
-84.482210	16.031454	1.721651
-85.265446	16.248041	1.726656
-85.309682	15.315909	1.731661
-86.172932	12.913932	1.736666
-86.649601	9.915526	1.741670
-86.465420	10.206514	1.746675
-86.653713	15.902746	1.751680
-86.984557	14.132259	1.756685
-86.571537	10.217103	1.761690
-86.777833	11.267964	1.766694
-86.560318	6.701434	1.771699
-87.451791	18.022649	1.776704
-87.555583	6.456887	1.781709
-88.356094	16.268642	1.786714
-89.416659	17.263066	1.791718
-88.819013	12.914182	1.796723
-89.182110	19.798889	1.801728
-89.282670	7.805761	1.806733
-89.277861	13.325759	1.811738
-89.751865	10.451035	1.816742
-89.380519	15.082716	1.821747
-90.220003	19.477653	1.826752
-90.663154	8.486685	1.831757
-90.667326	15.482635	1.836762
-91.333943	14.292270	1.841766
-91.051839	8.894141	1.846771
-91.117184	20.156675	1.851776
-91.740190	12.584079	1.856781
-92.171862	14.530464	1.861786
-92.547245	10.993144	1.866790
-92.502034	9.561550	1.871795
-92.472396	12.575464	1.876800
-92.897813	11.430398	1.881805
-93.019864	14.766421	1.886810
-94.058313	17.726951	1.891814
-94.142417	10.172055	1.896819
-94.467056	11.792284	1.901824
-94.323379	13.110778	1.906829
-94.402817	14.445703	1.911834
-94.747066	15.135010	1.916838
-94.018697	10.597729	1.921843
-95.352970	18.736111	1.926848
-95.602398	11.739420	1.931853
-95.943968	11.564364	1.936858
-96.599623	11.352529	1.941862
-96.082049	8.905571	1.946867
-96.375703	18.486564	1.951872
-96.170907	7.634946	1.956877
-96.812198	15.347556	1.961882
-97.454879	21.337691	1.966886
-97.469799	13.977744	1.971891
-97.693449	15.806994	1.976896
-98.021061	11.727584	1.981901
-97.941806	5.314629	1.986906
-98.601545	12.260304	1.991910
-98.973911	9.601599	1.996915
-99.325193	14.457160	2.006912
-98.650552	11.559754	2.016909
-98.047406	8.645936	2.026906
-97.976981	14.515652	2.036902
-97.357642	12.320731	2.046899
-96.795828	17.704409	2.056896
-96.501993	20.342774	2.066893
-95.151533	11.129870	2.076890
-95.251121	21.465696	2.086886
-95.007832	14.079676	2.096883
-94.121670	12.570440	2.106880
-93.656938	19.960271	2.116877
-93.387517	19.646023	2.126874
-92.494510	10.656086	2.136870
-92.067783	12.991475	2.146867
-91.735929	16.847383	2.156864
-91.556164	13.667595	2.166861
-90.554090	10.114709	2.176858
-90.542495	16.271382	2.186854
-89.527221	10.306371	2.196851
-88.949099	17.550572	2.206848
-88.866701	16.792306	2.216845
-88.787191	11.779533	2.226842
-87.874955	13.323799	2.236838
-86.561818	17.295581	2.246835
-86.631378	18.244521	2.256832
-86.355216	15.406001	2.266829
-86.114729	11.963051	2.276826
-85.278991	18.524214	2.286822
-84.943528	12.458206	2.296819
-83.803756	10.328440	2.306816
-83.288675	13.074795	2.316813
-83.264543	17.497563	2.326810
-82.982515	6.736311	2.336806
-82.066437	15.293603	2.346803
-81.891412	11.318927	2.356800
-81.101226	14.052715	2.366797
-80.004995	16.883412	2.376794
-80.324460	14.824812	2.386790
-80.064797	17.182341	2.396787
-79.145612	23.932015	2.406784
-78.323013	25.841646	2.416781
-78.487058	24.507929	2.426778
-77.778275	19.551371	2.436774
-76.894377	24.166849	2.446771
-76.916316	25.516311	2.456768
-76.358682	17.521235	2.466765
-75.725399	19.569509	2.476762
-75.116107	15.778385	2.486758
-74.196562	17.228975	2.496755
-73.823341	25.588303	2.506752
-73.819661	23.282944	2.516749
-73.815022	22.081136	2.526746
-72.652952	20.484319	2.536742
-72.242406	17.046002	2.546739
-71.435279	26.147121	2.556736
-70.911865	24.315640	2.566733
-70.562490	21.826178	2.576730
-70.458626	26.915831	2.586726
-69.863655	23.115026	2.596723
-69.073734	17.387492	2.606720
-68.441232	14.906266	2.616717
-67.983412	20.411499	2.626714
-67.407908	18.629481	2.636710
-67.606742	18.524575	2.646707
-66.942429	13.566890	2.656704
-66.413622	21.167212	2.666701
-65.070626	22.347914	2.676698
-64.853260	14.664672	2.686694
-64.340216	12.912956	2.696691
-64.276900	21.584816	2.706688
-64.202548	17.052236	2.716685
-63.326031	18.253489	2.726682
-62.767029	18.162963	2.736678
-61.929320	19.356813	2.746675
-61.506276	23.235757	2.756672
-61.364731	24.307012	2.766669
-60.207283	22.809361	2.776666
-60.123740	17.140331	2.786662
-59.885622	20.222022	2.796659
-59.219897	19.562559	2.806656
-58.474931	25.121007	2.816653
-58.244538	18.490708	2.826650
-57.473531	17.204852	2.836646
-56.884443	19.510987	2.846643
-57.167019	19.995909	2.856640
-56.005107	20.410536	2.866637
-55.271750	21.200024	2.876634
-55.373756	18.863168	2.886630
-54.674806	14.564422	2.896627
-53.865832	20.356088	2.906624
-53.744553	22.412302	2.916621
-53.199325	12.868441	2.926618
-52.299903	22.931137	2.936614
-52.028649	18.981027	2.946611
-51.783980	27.177698	2.956608
-51.455682	19.919264	2.966605
-50.637953	27.493872	2.976602
-49.922823	21.409439	2.986598
-49.065848	23.879859	2.996595
-48.856590	17.962588	3.006592
-48.659749	22.545054	3.016589
-48.581651	24.495401	3.026586
-47.593824	23.412716	3.036582
-47.257345	22.313425	3.046579
-46.598167	23.338076	3.056576
-46.157698	24.212823	3.066573
-45.938434	19.124146	3.076570
-44.690759	21.750365	3.086566
-44.380051	21.980544	3.096563
-44.256246	22.777132	3.106560
-43.684621	24.117600	3.116557
-42.814227	24.849028	3.126554
-42.538106	19.941406	3.136550
-42.453272	22.239572	3.146547
-41.412493	24.745349	3.156544
-41.017782	25.913185	3.166541
-40.916663	25.599151	3.176538
-39.481800	23.454904	3.186534
-39.166367	21.976377	3.196531
-39.248286	21.160956	3.206528
-39.287788	24.815585	3.216525
-38.244044	22.539120	3.226522
-37.463302	18.792514	3.236518
-36.632233	16.169538	3.246515
-36.383716	17.613309	3.256512
-36.467250	22.439795	3.266509
-36.090817	23.822074	3.276506
-35.319719	24.790255	3.286502
-33.931738	23.412500	3.296499
-33.571344	25.125229	3.306496
-33.903630	23.814630	3.316493
-33.434555	24.240866	3.326490
-32.617850	26.465248	3.336486
-32.058348	26.091305	3.346483
-31.336911	28.793419	3.356480
-30.792113	26.404174	3.366477
-30.607873	24.853126	3.376474
-30.019393	22.466923	3.386470
-29.587607	17.059911	3.396467
-28.828151	23.242903	3.406464
-28.736350	28.744941	3.416461
-28.410291	25.584195	3.426458
-27.311067	23.441398	3.436454
-27.100873	19.980544	3.446451
-26.410973	27.014200	3.456448
-25.620959	30.404013	3.466445
-25.272525	25.006259	3.476442
-25.335416	33.398899	3.486438
-24.805156	26.207586	3.496435
-24.015347	30.238795	3.506432
-23.910459	25.189409	3.516429
-23.070888	21.616816	3.526426
-22.500157	23.780574	3.536422
-21.933938	26.067977	3.546419
-21.321782	31.661076	3.556416
-21.097036	25.029734	3.566413
-20.535795	24.316054	3.576410
-20.000943	21.061060	3.586406
-19.307181	18.450354	3.596403
-19.149098	16.580786	3.606400
-18.715096	21.925976	3.616397
-17.838392	22.884377	3.626394
-17.582596	20.056147	3.636390
-17.010332	23.762592	3.646387
-16.473789	25.636426	3.656384
-16.008452	28.921349	3.666381
-15.697498	25.022161	3.676378
-14.904056	26.171981	3.686374
-14.457745	23.435690	3.696371
-14.272994	21.777269	3.706368
-13.241157	17.311566	3.716365
-12.900647	21.719091	3.726362
-12.869925	20.012283	3.736358
-11.934224	19.242519	3.746355
-11.601411	23.804448	3.756352
-11.028297	24.974751	3.766349
-9.982696	23.987227	3.776346
-9.980016	24.796959	3.786342
-9.942238	26.149177	3.796339
-9.027169	28.525025	3.806336
-8.316262	24.947858	3.816333
-8.180945	31.046709	3.826330
-7.328105	23.797235	3.836326
-6.751706	23.529565	3.846323
-6.903998	27.306607	3.856320
-6.215830	24.298101	3.866317
-5.352724	15.578282	3.876314
-4.977161	21.583009	3.886310
-4.053200	28.434264	3.896307
-3.672831	21.724989	3.906304
-3.641781	27.837550	3.916301
-3.660614	31.821888	3.926298
-3.189209	34.919684	3.936294
-2.313975	57.415520	3.946291
-1.650488	69.126470	3.956288
-1.165749	88.166045	3.966285
-1.181477	94.801486	3.976282
-0.648235	114.224873	3.986278
0.000000	122.760346	3.991283
0.087914	128.845802	3.996288
-0.005236	139.391585	4.001293
0.769614	151.280346	4.006298
0.695850	158.324793	4.011302
0.528916	162.812029	4.016307
0.966830	158.869236	4.021312
0.603066	169.988117	4.026317
1.111703	169.076700	4.031322
0.845165	173.091439	4.036326
0.832596	173.648660	4.041331
1.017527	177.419916	4.046336
0.783284	175.299515	4.051341
0.922480	175.865742	4.056346
0.899591	177.049039	4.061350
1.031288	175.882138	4.066355
0.781248	174.063117	4.071360
0.794604	170.473014	4.076365
0.626308	169.358753	4.081370
0.937788	173.977518	4.086374
0.768793	158.592368	4.091379
0.833289	167.582133	4.096384
1.168752	176.424417	4.101389
0.860015	165.807698	4.106394
0.670121	169.313054	4.111398
1.227238	163.295284	4.116403
0.932766	176.098979	4.121408
0.746710	178.579932	4.126413
1.167654	166.176085	4.131418
0.786068	180.024293	4.136422
1.071870	167.336563	4.141427
0.912438	171.635881	4.146432
0.742924	171.089355	4.151437
0.969922	172.443600	4.156442
0.620284	181.322578	4.161446
1.103529	194.291327	4.166451
1.153079	201.334711	4.171456
1.115026	207.607610	4.176461
1.272574	193.144168	4.181466
1.167741	201.909012	4.186470
1.260192	196.010409	4.191475
1.586418	200.962801	4.196480
1.062408	196.175850	4.201485
1.395002	187.646678	4.206490
1.336083	193.276755	4.211494
1.316323	182.372606	4.216499
1.135816	166.543576	4.221504
1.000543	176.396810	4.226509
1.233074	180.547748	4.231514
1.288874	196.965451	4.236518
1.399653	202.581440	4.241523
1.226952	208.459471	4.246528
1.589913	201.189784	4.251533
1.693841	193.871432	4.256538
1.068736	199.175149	4.261542
1.065453	198.437109	4.266547
1.184642	199.295548	4.271552
1.236495	206.362431	4.276557
1.631188	195.089690	4.281562
1.314624	202.080829	4.286566
1.506737	202.316442	4.291571
1.620917	203.737918	4.296576
1.193982	204.212207	4.301581
1.322149	203.284664	4.306586
1.152410	202.440001	4.311590
1.247595	200.064748	4.316595
1.848169	198.470719	4.321600
1.785920	203.396867	4.326605
1.752558	193.938662	4.331610
1.472908	199.933463	4.336614
1.571738	199.380978	4.341619
1.634398	198.059155	4.346624
1.554234	200.107778	4.351629
1.766414	199.322413	4.356634
1.601609	203.457855	4.361638
1.219293	198.289078	4.366643
1.664410	197.488425	4.371648
1.445685	195.170090	4.376653
1.724681	198.225235	4.381658
1.635736	207.829280	4.386662
1.609445	197.238780	4.391667
1.831515	197.758724	4.396672
1.438211	203.806882	4.401677
2.073512	198.143983	4.406682
1.705842	202.402017	4.411686
1.757098	205.902967	4.416691
1.695085	196.099631	4.421696
1.685196	199.303257	4.426701
1.861037	193.213245	4.431706
1.595127	191.164390	4.436710
1.653813	194.267859	4.441715
1.788176	200.878849	4.446720
1.723006	209.273441	4.451725
1.830163	192.592213	4.456730
1.551396	201.400068	4.461734
1.732215	207.888322	4.466739
2.018390	222.106495	4.471744
1.683669	224.987010	4.476749
1.902213	226.696877	4.481754
1.852459	229.938488	4.486758
1.758207	229.058037	4.491763
2.122486	231.610860	4.496768
1.905502	236.235857	4.501773
2.073681	233.451472	4.506778
1.941915	231.922082	4.511782
2.070344	228.681334	4.516787
2.000724	226.570762	4.521792
1.940923	230.024988	4.526797
2.028145	225.980807	4.531802
1.881340	233.823369	4.536806
2.020890	234.492550	4.541811
2.062575	226.624651	4.546816
1.695455	237.395248	4.551821
2.015579	229.238122	4.556826
1.620379	234.327360	4.561830
1.901709	230.973082	4.566835
2.153176	219.528482	4.571840
1.882567	224.599453	4.576845
2.279118	234.786752	4.581850
2.216610	248.728209	4.586854
2.486602	238.280623	4.591859
2.538901	234.133294	4.596864
1.721182	229.131529	4.601869
1.839668	239.359354	4.606874
2.272791	254.817942	4.611878
2.428717	252.394142	4.616883
2.518531	261.990916	4.621888
2.137038	247.586301	4.626893
2.311934	240.693470	4.631898
2.306270	254.423448	4.636902
2.312856	264.923200	4.641907
2.373599	263.949986	4.646912
2.194611	269.452762	4.651917
2.369114	262.516376	4.656922
2.039010	264.469644	4.661926
2.546622	261.605166	4.666931
2.606029	267.766834	4.671936
2.615527	256.607565	4.676941
2.462773	263.243239	4.681946
2.633905	263.012472	4.686950
2.346754	255.776023	4.691955
2.436349	242.070309	4.696960
2.225730	261.004611	4.701965
2.383395	262.332655	4.706970
2.586058	260.639542	4.711974
2.590701	270.888807	4.716979
2.514704	255.124865	4.721984
2.888487	262.761449	4.726989
2.671144	242.379206	4.731994
2.412520	240.466878	4.736998
2.439441	233.250654	4.742003
2.179044	249.676573	4.747008
2.710031	253.555314	4.752013
2.765602	256.905783	4.757018
2.644617	261.396488	4.762022
2.586881	259.166135	4.767027
2.570314	262.586371	4.772032
2.390704	269.030737	4.777037
2.450074	262.792645	4.782042
2.571749	272.980300	4.787046
2.625633	264.195516	4.792051
2.479162	271.212391	4.797056
2.115137	271.862943	4.802061
2.459095	269.433261	4.807066
2.330516	267.865845	4.812070
2.570899	273.216491	4.817075
2.824881	282.236315	4.822080
3.034905	289.191202	4.827085
2.972078	283.176001	4.832090
2.707076	281.985394	4.837094
2.409548	280.251777	4.842099
3.041070	285.430698	4.847104
2.806680	291.834022	4.852109
3.007634	287.939318	4.857114
2.867297	293.005906	4.862118
2.973774	290.449983	4.867123
3.202180	295.106222	4.872128
2.631402	284.199319	4.877133
2.959672	289.253029	4.882138
3.301270	283.695965	4.887142
3.085682	283.328746	4.892147
3.416793	273.221878	4.897152
2.950673	270.460042	4.902157
3.178511	276.295251	4.907162
2.849610	271.313164	4.912166
2.703140	264.275614	4.917171
3.105461	262.528914	4.922176
3.005793	268.896106	4.927181
2.732862	271.413956	4.932186
2.820108	278.194202	4.937190
3.330975	281.898483	4.942195
3.247649	274.365421	4.947200
2.889698	272.835200	4.952205
3.078278	259.263053	4.957210
2.955724	275.713138	4.962214
3.088719	278.650791	4.967219
3.081854	294.838818	4.972224
2.729051	280.720097	4.977229
3.204589	280.783072	4.982234
3.083668	291.564638	4.987238
3.120607	290.568724	4.992243
3.450008	287.522407	4.997248
3.071818	294.301988	5.002253
3.404504	289.790895	5.007258
3.147128	297.804341	5.012262
2.829227	300.110600	5.017267
3.228409	289.705719	5.022272
3.266513	290.139507	5.027277
3.199905	278.992234	5.032282
3.199356	292.957609	5.037286
2.681408	296.862263	5.042291
2.980773	287.264244	5.047296
3.271233	297.228009	5.052301
3.296986	311.903204	5.057306
3.439655	324.137737	5.062310
3.464038	314.378825	5.067315
3.030134	313.269072	5.072320
3.330697	316.229500	5.077325
3.411095	310.390670	5.082330
3.343070	323.428520	5.087334
3.309422	317.916614	5.092339
3.435789	319.398638	5.097344
3.007548	325.039011	5.102349
3.928918	325.426578	5.107354
3.465732	327.160946	5.112358
3.304430	324.390259	5.117363
3.736894	316.579358	5.122368
3.441433	327.361633	5.127373
3.483867	321.552963	5.132378
3.487336	324.319080	5.137382
3.553722	325.656128	5.142387
3.765519	324.816554	5.147392
3.215606	321.258126	5.152397
3.848912	324.058667	5.157402
3.709095	322.907513	5.162406
3.715371	321.420967	5.167411
3.462783	319.943742	5.172416
3.603993	325.445807	5.177421
3.768289	318.966142	5.182426
3.349758	321.710579	5.187430
3.536987	324.559141	5.192435
3.547735	319.809691	5.197440
3.407035	321.913742	5.202445
3.402793	320.074719	5.207450
3.592616	333.363908	5.212454
3.766093	340.760589	5.217459
3.976393	345.702822	5.222464
3.775108	354.644948	5.227469
3.962948	349.540360	5.232474
3.869039	341.432006	5.237478
3.893413	332.965439	5.242483
3.848615	330.932045	5.247488
3.721049	327.188824	5.252493
4.121465	326.097787	5.257498
3.743031	332.923009	5.262502
3.816895	323.250421	5.267507
3.585446	321.043893	5.272512
3.995789	345.153615	5.277517
4.116629	347.346375	5.282522
4.254493	352.489655	5.287526
3.757335	337.346338	5.292531
3.960836	333.745231	5.297536
3.683752	342.554072	5.302541
4.225193	344.972198	5.307546
4.270677	353.067734	5.312550
3.874183	335.197727	5.317555
3.485732	342.828560	5.322560
3.993546	352.440235	5.327565
4.307188	351.236284	5.332570
4.134285	347.516155	5.337574
4.138579	356.059363	5.342579
4.192992	352.541353	5.347584
4.094733	348.787749	5.352589
4.102019	341.937824	5.357594
4.024302	345.067859	5.362598
3.861815	355.269868	5.367603
4.174210	354.996762	5.372608
4.194908	355.292930	5.377613
4.033084	346.603416	5.382618
3.908388	348.093077	5.387622
3.905557	345.074338	5.392627
3.974510	346.036419	5.397632
3.681706	359.179604	5.402637
3.996543	344.985979	5.407642
3.786792	354.937501	5.412646
4.115668	372.171147	5.417651
4.342459	386.302611	5.422656
4.069898	382.827099	5.427661
4.645614	388.251706	5.432666
4.305086	394.493665	5.437670
4.230338	395.680435	5.442675
4.041073	390.560531	5.447680
4.098323	394.562359	5.452685
4.512568	390.405173	5.457690
4.326831	392.075841	5.462694
4.195238	387.407762	5.467699
4.277069	388.659968	5.472704
3.988814	393.950986	5.477709
4.186701	388.637123	5.482714
4.203535	392.552697	5.487718
4.170571	393.668807	5.492723
4.120018	386.301946	5.497728
4.241734	407.927533	5.502733
4.594844	421.661985	5.507738
4.504456	424.827681	5.512742
4.424854	418.356199	5.517747
4.526931	416.719787	5.522752
4.494882	426.030576	5.527757
4.824981	420.655340	5.532762
4.692574	422.967801	5.537766
4.502936	418.731429	5.542771
4.672606	423.592798	5.547776
4.654839	423.722470	5.552781
4.985043	429.364958	5.557786
4.521289	415.986741	5.562790
4.321154	400.827130	5.567795
5.092543	412.561363	5.572800
4.544686	413.546855	5.577805
4.444231	404.496280	5.582810
4.676672	421.885469	5.587814
4.498535	421.622948	5.592819
4.525045	420.777940	5.597824
4.558825	431.276458	5.602829
4.668030	427.782708	5.607834
4.547599	414.505705	5.612838
4.453197	425.029393	5.617843
4.747013	420.649417	5.622848
4.860307	424.374579	5.627853
5.018760	420.362558	5.632858
4.594640	427.737473	5.637862
4.733171	421.650787	5.642867
4.919270	421.422276	5.647872
4.608416	427.099093	5.652877
5.093867	418.858050	5.657882
4.663320	429.262764	5.662886
4.417650	425.925464	5.667891
4.853329	419.635648	5.672896
4.572012	426.869696	5.677901
4.932547	436.062789	5.682906
5.026987	448.233971	5.687910
5.076731	447.320190	5.692915
4.762440	434.887318	5.697920
4.766553	455.521091	5.702925
5.183367	455.139522	5.707930
5.436490	460.677568	5.712934
5.031986	443.120556	5.717939
4.747640	437.696301	5.722944
5.096937	453.697638	5.727949
5.127078	450.864835	5.732954
4.884026	448.349601	5.737958
5.085250	446.605004	5.742963
5.100984	448.993381	5.747968
4.727174	463.820533	5.752973
4.810758	463.694248	5.757978
5.104658	464.299594	5.762982
4.842295	466.129976	5.767987
5.136440	450.713423	5.772992
5.130702	467.110621	5.777997
5.044676	457.916726	5.783002
5.078567	465.051823	5.788006
5.010630	466.778572	5.793011
5.210104	457.464185	5.798016
5.214964	469.939713	5.803021
5.313281	459.628746	5.808026
5.172838	458.147145	5.813030
5.226616	466.450741	5.818035
4.959240	455.755734	5.823040
4.812843	462.018261	5.828045
5.183692	482.733816	5.833050
5.326459	493.864163	5.838054
5.075196	498.359343	5.843059
5.739108	506.219540	5.848064
5.535650	499.287818	5.853069
5.501306	488.759430	5.858074
5.344194	486.982605	5.863078
4.980290	479.135173	5.868083
5.358468	479.802736	5.873088
5.172357	495.773589	5.878093
5.302987	492.395665	5.883098
5.164355	493.919222	5.888102
5.122349	496.279082	5.893107
5.240140	497.024104	5.898112
5.157830	491.462375	5.903117
5.410496	496.094134	5.908122
5.460032	486.552559	5.913126
5.389582	493.683242	5.918131
5.518992	495.028812	5.923136
5.252988	498.223606	5.928141
5.634460	495.498181	5.933146
5.544808	496.907656	5.938150
5.483229	506.566161	5.943155
6.054493	514.591485	5.948160
5.599890	503.312938	5.953165
5.648847	501.036267	5.958170
5.771329	495.313340	5.963174
5.657442	495.434460	5.968179
5.611047	486.877702	5.973184
5.428186	504.630187	5.978189
5.884512	496.125547	5.983194
5.621448	498.378747	5.988198
5.454743	498.041317	5.993203
5.676242	506.459244	5.998208
5.496014	518.626237	6.003213
6.128134	513.974126	6.008218
5.725255	512.158273	6.013222
5.661045	512.068895	6.018227
5.821358	497.574125	6.023232
5.521706	504.479124	6.028237
5.660305	494.138572	6.033242
5.693800	502.513827	6.038246
5.380724	493.668713	6.043251
5.902681	516.036073	6.048256
5.841232	530.607512	6.053261
5.828401	513.035092	6.058266
5.828423	506.970915	6.063270
5.282765	504.939928	6.068275
5.543474	513.036611	6.073280
5.472896	523.234561	6.078285
5.779472	523.798343	6.083290
6.028048	536.865641	6.088294
5.895594	523.916144	6.093299
5.806303	508.809310	6.098304
5.656049	507.180930	6.103309
5.808911	499.184564	6.108314
5.575421	502.939743	6.113318
5.468389	492.995276	6.118323
5.689291	510.621900	6.123328
5.775015	523.223401	6.128333
5.567469	510.667016	6.133338
5.926933	517.014715	6.138342
5.520126	519.553591	6.143347
5.771762	509.778037	6.148352
5.511228	509.795172	6.153357
6.008788	518.344402	6.158362
5.866262	515.865791	6.163366
5.726503	500.251479	6.168371
5.996307	498.720091	6.173376
5.784556	501.477677	6.178381
5.855661	494.069502	6.183386
5.697988	494.100389	6.188390
5.599194	497.542976	6.193395
5.775403	494.416215	6.198400
5.284086	489.579553	6.203405
5.383702	489.116519	6.208410
5.619548	510.610668	6.213414
5.421032	513.436711	6.218419
6.220103	520.925836	6.223424
5.630859	509.874813	6.228429
5.590592	502.253403	6.233434
5.505774	513.585243	6.238438
5.767254	519.875957	6.243443
5.994837	507.579441	6.248448
5.887851	504.909447	6.253453
5.817006	497.626210	6.258458
5.692907	508.749059	6.263462
5.403737	506.800314	6.268467
5.917101	499.707261	6.273472
5.518827	501.774660	6.278477
5.836137	503.321777	6.283482
5.433056	497.979325	6.288486
5.582295	499.623935	6.293491
5.549238	507.269602	6.298496
6.000300	519.835267	6.303501
5.969822	509.200056	6.308506
5.866682	506.132972	6.313510
5.471910	505.130391	6.318515
5.934505	497.028466	6.323520
5.707811	503.902045	6.328525
5.875988	496.654806	6.333530
5.629046	503.225468	6.338534
5.482744	499.122206	6.343539
5.916555	488.959314	6.348544
5.797286	503.623383	6.353549
5.585598	497.662155	6.358554
5.801623	492.656849	6.363558
5.458264	495.200211	6.368563
5.879893	492.953984	6.373568
5.950272	501.658210	6.378573
5.901962	496.641226	6.383578
5.923773	511.860338	6.388582
5.439865	503.461471	6.393587
5.514320	500.560344	6.398592
5.523986	507.032074	6.403597
5.605712	511.956975	6.408602
5.787273	506.788647	6.413606
5.514623	499.611449	6.418611
5.683634	495.253305	6.423616
5.489911	501.038232	6.428621
5.612746	499.571045	6.433626
5.402171	497.992122	6.438630
5.480622	512.669437	6.443635
6.158943	526.807953	6.448640
5.626341	517.449591	6.453645
5.902759	510.048652	6.458650
5.674967	509.324688	6.463654
5.351486	510.814525	6.468659
5.762067	508.060597	6.473664
5.839416	518.340215	6.478669
5.850435	510.305567	6.483674
5.589544	506.073472	6.488678
5.620289	508.712952	6.493683
6.089610	499.365102	6.498688
5.524545	501.505115	6.503693
5.928550	506.479852	6.508698
5.835436	508.024289	6.513702
5.683567	506.607921	6.518707
5.669501	493.143722	6.523712
5.842935	507.635197	6.528717
5.553882	502.633805	6.533722
5.802868	500.066878	6.538726
6.015366	509.987056	6.543731
6.046717	497.656343	6.548736
5.480574	500.472814	6.553741
5.771501	500.153532	6.558746
5.546069	498.727244	6.563750
5.648923	493.679110	6.568755
5.786285	499.903344	6.573760
5.526917	508.374658	6.578765
5.752657	503.660393	6.583770
5.671956	501.729224	6.588774
5.576517	500.407508	6.593779
5.988118	498.984855	6.598784
5.869354	500.107683	6.603789
5.589201	506.853755	6.608794
5.837178	502.302164	6.613798
5.900786	501.143752	6.618803
6.007911	505.274894	6.623808
5.463680	509.384448	6.628813
5.916825	502.186909	6.633818
5.566469	503.832752	6.638822
5.517624	508.890179	6.643827
5.888611	505.443638	6.648832
5.778547	498.493885	6.653837
5.727938	506.223367	6.658842
6.060892	505.148818	6.663846
5.936369	507.012225	6.668851
6.094508	500.283279	6.673856
5.420840	499.611051	6.678861
5.671681	491.359093	6.683866
5.509543	491.767239	6.688870
5.476934	506.079314	6.693875
5.883863	505.666228	6.698880
5.901995	505.059606	6.703885
5.734792	502.920756	6.708890
6.134586	499.903985	6.713894
5.626244	488.602773	6.718899
5.580623	480.150678	6.723904
5.291361	486.006675	6.728909
5.522823	486.356745	6.733914
5.757649	502.689476	6.738918
5.704103	491.872402	6.743923
5.745934	510.932545	6.748928
5.776490	506.513260	6.753933
5.619778	500.296253	6.758938
5.570214	510.594120	6.763942
5.700318	505.459574	6.768947
5.856732	501.982657	6.773952
5.716175	513.128954	6.778957
5.948940	508.630202	6.783962
5.907622	501.642423	6.788966
5.576947	489.758255	6.793971
5.742765	483.531257	6.798976
5.621915	489.411069	6.803981
5.838492	499.220056	6.808986
5.803644	484.984555	6.813990
5.601011	483.509106	6.818995
5.914186	478.545339	6.824000
5.512466	477.848403	6.829005
5.637031	471.844129	6.834010
5.663799	480.191477	6.839014
5.695474	487.810627	6.844019
5.868617	479.108193	6.849024
5.480464	481.170756	6.854029
5.685099	490.227882	6.859034
5.535686	494.671463	6.864038
5.415208	495.836015	6.869043
5.673431	494.285628	6.874048
5.502931	507.362902	6.879053
6.195903	498.343880	6.884058
5.879824	505.225552	6.889062
5.879463	510.601545	6.894067
5.938807	489.393670	6.899072
5.483701	484.307103	6.904077
5.688157	481.179021	6.909082
5.517533	477.196616	6.914086
5.217625	493.434760	6.919091
5.824766	492.771842	6.924096
5.806191	509.775658	6.929101
5.719463	500.047659	6.934106
5.744944	497.568263	6.939110
5.448983	506.227779	6.944115
5.673457	507.903346	6.949120
5.768002	517.679665	6.954125
5.943079	499.979446	6.959130
5.948041	503.995683	6.964134
5.874461	492.871513	6.969139
5.600963	479.952316	6.974144
5.381731	477.117391	6.979149
5.725103	491.238525	6.984154
5.999757	490.342947	6.989158
5.642907	498.635035	6.994163
5.718994	471.222464	6.999168
5.470690	494.230625	7.004173
5.591644	494.334759	7.009178
5.697095	495.253311	7.014182
5.868755	501.891604	7.019187
5.895134	488.470441	7.024192
5.558452	486.966671	7.029197
5.659895	484.375240	7.034202
5.848815	488.177880	7.039206
5.263838	486.314434	7.044211
5.676163	494.651814	7.049216
5.450006	495.922077	7.054221
5.302967	499.003236	7.059226
5.738884	503.534991	7.064230
5.574370	504.988242	7.069235
5.563960	490.775527	7.074240
5.606087	505.555546	7.079245
5.563417	504.129382	7.084250
5.457427	504.422852	7.089254
5.448919	508.728647	7.094259
5.952983	500.396071	7.099264
5.410997	511.005581	7.104269
5.606013	505.253667	7.109274
5.689445	505.037815	7.114278
5.332275	503.915537	7.119283
5.965916	502.066962	7.124288
5.414282	506.854612	7.129293
5.542958	501.328587	7.134298
6.045909	515.123756	7.139302
5.524689	514.072453	7.144307
5.644099	505.656360	7.149312
5.573863	509.588553	7.154317
5.920287	524.193875	7.159322
5.703941	516.346853	7.164326
5.765361	512.435337	7.169331
5.827187	499.602086	7.174336
5.375032	508.250173	7.179341
5.702434	513.351264	7.184346
5.460936	514.548489	7.189350
5.468698	543.068214	7.194355
6.002932	534.378572	7.199360
5.266675	553.482567	7.204365
5.383601	544.678500	7.209370
5.915803	537.788135	7.214374
5.362097	554.658810	7.219379
6.046204	546.934194	7.224384
5.700113	541.159392	7.229389
5.816766	536.283604	7.234394
5.692551	535.126100	7.239398
5.737574	551.266334	7.244403
6.209477	532.575418	7.249408
5.771713	541.136876	7.254413
5.793012	521.997251	7.259418
5.926839	510.903250	7.264422
5.870241	505.667800	7.269427
5.733001	495.498829	7.274432
5.657850	503.683884	7.279437
5.754378	501.512213	7.284442
5.662866	496.157632	7.289446
5.372505	497.611002	7.294451
6.058442	497.653346	7.299456
5.598472	500.574584	7.304461
5.653099	492.582057	7.309466
5.800491	502.774880	7.314470
5.484166	500.128898	7.319475
5.535790	498.922544	7.324480
5.478769	503.270313	7.329485
5.906875	514.846768	7.334490
5.853061	509.227230	7.339494
5.688561	505.867985	7.344499
5.958974	497.345587	7.349504
5.366820	504.119447	7.354509
5.820880	504.158749	7.359514
5.925294	502.175612	7.364518
5.648453	505.501655	7.369523
5.883409	497.363623	7.374528
5.940637	503.314988	7.379533
5.659146	497.077994	7.384538
5.760202	503.376915	7.389542
5.740249	505.220439	7.394547
5.953735	498.631319	7.399552
5.773951	512.041861	7.404557
5.699144	507.886104	7.409562
5.490974	504.899365	7.414566
5.374253	498.135423	7.419571
5.685765	492.498412	7.424576
5.785333	503.607109	7.429581
5.783645	502.689409	7.434586
5.835229	497.390462	7.439590
5.554454	501.885596	7.444595
5.683444	507.380475	7.449600
5.717005	508.629437	7.454605
5.964938	502.868563	7.459610
6.044690	509.825586	7.464614
5.825746	511.025193	7.469619
5.809816	501.982271	7.474624
5.592587	506.651986	7.479629
5.681407	504.022582	7.484634
5.542908	498.636907	7.489638
5.504381	502.432617	7.494643
5.533022	499.637943	7.499648
5.433753	506.037135	7.504653
5.812382	502.828503	7.509658
5.888547	511.708394	7.514662
5.669390	513.229896	7.519667
6.034511	503.341620	7.524672
5.809312	513.058996	7.529677
5.557384	509.618717	7.534682
5.867985	506.319721	7.539686
5.657262	507.200251	7.544691
5.428423	503.590385	7.549696
5.634923	502.156506	7.554701
5.686740	502.573031	7.559706
6.190474	503.684338	7.564710
5.786857	502.986727	7.569715
5.875797	497.940501	7.574720
5.505215	510.111186	7.579725
5.848315	509.951792	7.584730
5.844041	508.159916	7.589734
5.477537	505.528557	7.594739
5.929417	501.524954	7.599744
5.419728	506.637778	7.604749
5.542308	510.347610	7.609754
5.941055	503.486858	7.614758
5.581331	512.300007	7.619763
5.910548	510.498490	7.624768
5.621070	509.336190	7.629773
5.450643	501.542746	7.634778
5.739237	503.161516	7.639782
5.627884	504.235164	7.644787
5.880303	501.257401	7.649792
5.584248	510.059216	7.654797
5.934923	501.935566	7.659802
5.786364	507.640001	7.664806
5.589655	509.645211	7.669811
5.856485	501.761398	7.674816
5.739290	506.256283	7.679821
5.701219	504.250564	7.684826
5.886881	504.685576	7.689830
5.670679	508.118402	7.694835
5.679462	502.833250	7.699840
5.745576	505.861155	7.704845
5.772624	506.439060	7.709850
5.781997	500.898850	7.714854
5.548633	512.447694	7.719859
5.643358	504.704864	7.724864
5.469857	511.470770	7.729869
5.747880	506.747846	7.734874
5.694323	505.209226	7.739878
5.544710	508.677992	7.744883
6.086755	500.609678	7.749888
5.950765	508.987743	7.754893
5.857272	507.913562	7.759898
5.799487	510.544614	7.764902
5.700334	501.437723	7.769907
5.550842	491.309067	7.774912
5.590726	504.056083	7.779917
5.708773	507.927692	7.784922
5.856982	507.618625	7.789926
5.567216	512.003361	7.794931
5.533167	509.013835	7.799936
5.611049	510.820437	7.804941
5.592157	515.847449	7.809946
6.061359	509.871734	7.814950
5.670491	506.466896	7.819955
5.669252	500.396024	7.824960
5.791796	506.396762	7.829965
5.850148	498.828288	7.834970
5.507047	502.897429	7.839974
5.373151	504.270620	7.844979
5.730386	503.135414	7.849984
5.620458	503.327907	7.854989
5.816747	509.060090	7.859994
5.854867	503.082356	7.864998
5.649958	516.232627	7.870003
5.551957	504.102317	7.875008
5.873487	502.130389	7.880013
5.537332	511.963821	7.885018
5.736573	499.809944	7.890022
5.452193	505.295920	7.895027
5.583899	500.288591	7.900032
5.493058	505.735611	7.905037
5.691601	506.136915	7.910042
5.671993	504.902495	7.915046
5.700110	509.609530	7.920051
5.593249	513.139102	7.925056
5.726899	512.531899	7.930061
5.869774	515.515520	7.935066
5.870154	513.380688	7.940070
5.743688	516.270972	7.945075
5.813678	507.039174	7.950080
5.712659	513.534564	7.955085
5.588563	498.783188	7.960090
5.919610	508.581314	7.965094
5.820557	507.306176	7.970099
6.047025	505.642051	7.975104
5.596024	519.887064	7.980109
5.698737	518.565488	7.985114
5.757951	512.564917	7.990118
5.486488	516.474124	7.995136
5.761518	512.040375	8.000154
5.755371	517.570138	8.005171
5.461985	505.294523	8.010189
5.853358	500.756479	8.015206
5.428269	510.582057	8.020224
5.785354	510.208616	8.025242
6.007467	507.264422	8.030259
5.723445	505.966719	8.035277
6.068024	499.057279	8.040294
5.778824	503.056672	8.045312
5.834725	499.635714	8.050330
5.734544	485.803633	8.055347
5.700950	499.786872	8.060365
5.618270	485.563145	8.065382
5.218937	503.832013	8.070400
5.680158	500.506124	8.075418
5.594835	514.816029	8.080435
5.454473	500.380203	8.085453
5.927350	501.056008	8.090470
5.391095	515.566956	8.095488
5.469608	513.883060	8.100506
5.357317	512.028612	8.105523
5.479965	518.976304	8.110541
5.980895	523.342848	8.115558
6.004730	534.418997	8.120576
5.917103	513.034603	8.125594
5.880371	518.711743	8.130611
6.016902	514.819196	8.135629
5.992772	505.225750	8.140646
5.831794	514.697775	8.145664
5.847298	508.448488	8.150682
5.808853	510.668895	8.155699
5.476791	511.752977	8.160717
5.878234	521.586558	8.165734
6.260858	526.802159	8.170752
6.044035	514.800647	8.175770
5.757715	516.347985	8.180787
5.494798	510.790029	8.185805
5.894490	510.851428	8.190822
5.865975	538.803253	8.195840
6.055265	535.893031	8.200858
5.751144	538.605435	8.205875
5.941393	541.568623	8.210893
6.178528	535.615669	8.215910
5.920229	528.158072	8.220928
5.861926	512.997086	8.225946
5.739290	526.498283	8.230963
6.204396	525.570184	8.235981
6.264215	520.353237	8.240998
5.779576	515.911048	8.246016
5.783771	498.762714	8.251034
5.914097	519.882635	8.256051
6.168552	534.836433	8.261069
6.009068	524.523517	8.266086
5.902236	521.723945	8.271104
6.019215	506.997879	8.276122
6.175246	514.657111	8.281139
5.848536	510.181488	8.286157
6.009686	499.571021	8.291174
6.024450	507.823482	8.296192
6.222154	517.014867	8.301210
6.117480	509.352325	8.306227
5.937768	510.890669	8.311245
6.101571	500.403966	8.316262
5.412976	512.851327	8.321280
5.789611	531.918229	8.326298
6.144417	543.919225	8.331315
5.881468	548.284530	8.336333
6.241194	540.089786	8.341350
6.215388	543.865860	8.346368
6.023902	548.271689	8.351386
6.042761	550.001349	8.356403
6.088805	552.912638	8.361421
6.021144	549.062755	8.366438
6.107734	554.574811	8.371456
6.272333	543.838162	8.376474
6.358885	540.487900	8.381491
6.006389	552.143273	8.386509
6.336729	542.596213	8.391526
5.946357	538.366735	8.396544
5.991122	537.162602	8.401562
6.053346	545.506034	8.406579
5.858711	551.814407	8.411597
6.262848	553.425150	8.416614
6.222167	554.571998	8.421632
6.367956	541.751221	8.426650
6.148319	540.066503	8.431667
6.057768	550.509884	8.436685
6.047297	552.078862	8.441702
6.072118	551.464206	8.446720
5.955965	544.948540	8.451738
6.323569	546.798780	8.456755
6.135571	555.475168	8.461773
6.102194	548.741477	8.466790
5.858580	544.200708	8.471808
6.134216	548.089057	8.476826
5.943847	544.747647	8.481843
5.968597	555.074306	8.486861
5.867256	541.406726	8.491878
5.800638	550.632456	8.496896
6.092734	547.101708	8.501914
6.441461	564.492691	8.506931
6.017390	563.852774	8.511949
6.429977	562.855423	8.516966
5.972564	571.638242	8.521984
6.130379	566.082635	8.527002
6.406439	578.248064	8.532019
6.300579	588.949499	8.537037
6.328167	579.046086	8.542054
6.260389	582.383090	8.547072
6.167971	580.363740	8.552090
6.099956	578.643083	8.557107
6.195069	579.843818	8.562125
6.317791	582.539477	8.567143
6.199406	580.041982	8.572160
6.350698	584.687491	8.577178
6.366440	585.086863	8.582195
6.427858	584.137429	8.587213
6.390184	577.223742	8.592231
5.900931	578.498218	8.597248
6.317567	585.702155	8.602266
6.153621	580.555313	8.607283
6.006139	589.649585	8.612301
6.451536	580.036996	8.617319
6.453153	578.262881	8.622336
6.318219	578.219916	8.627354
6.361754	577.924381	8.632371
6.117320	584.500641	8.637389
6.098966	577.942389	8.642407
6.524436	582.275190	8.647424
6.477578	584.498969	8.652442
6.442505	569.184289	8.657459
6.396827	588.734749	8.662477
6.581212	572.230068	8.667495
6.325789	581.120967	8.672512
6.401647	584.416273	8.677530
6.372226	579.653620	8.682547
6.303812	590.962589	8.687565
6.094662	581.989259	8.692583
5.873596	597.761574	8.697600
6.492869	608.553947	8.702618
6.881727	607.511905	8.707635
6.663004	617.503952	8.712653
6.622370	596.597453	8.717671
6.457528	582.295124	8.722688
6.389834	596.972236	8.727706
6.377437	595.087850	8.732723
6.303063	594.718934	8.737741
6.523082	603.869080	8.742759
6.557258	619.983571	8.747776
6.497045	619.822727	8.752794
6.827818	610.577304	8.757811
6.665506	609.325180	8.762829
6.438901	593.348149	8.767847
6.345583	597.151951	8.772864
6.536364	606.001057	8.777882
6.891961	605.020031	8.782899
6.308714	591.327887	8.787917
6.548390	592.675930	8.792935
6.478510	596.649066	8.797952
6.815011	609.626696	8.802970
6.696310	585.624897	8.807987
6.296297	591.541935	8.813005
6.595898	595.438136	8.818023
6.750215	609.837174	8.823040
6.606742	598.201180	8.828058
6.854092	598.753915	8.833075
6.444102	600.035148	8.838093
6.247794	595.815640	8.843111
6.677032	596.351837	8.848128
6.660459	614.493674	8.853146
6.918492	613.834098	8.858163
6.680224	607.881305	8.863181
6.527707	601.983601	8.868199
6.512071	607.873209	8.873216
6.435604	614.498431	8.878234
6.708250	600.617499	8.883251
6.652165	614.272109	8.888269
6.589299	613.670398	8.893287
6.487994	606.320023	8.898304
6.695479	616.301326	8.903322
6.745117	612.175328	8.908339
6.409319	612.547292	8.913357
6.608116	611.799106	8.918375
6.556458	613.011158	8.923392
6.512836	613.198329	8.928410
6.882552	607.072615	8.933427
6.604556	610.659382	8.938445
6.666250	606.425491	8.943463
6.894272	609.501917	8.948480
6.448103	618.450014	8.953498
6.772983	607.939123	8.958515
6.698519	606.750004	8.963533
6.745122	614.869109	8.968551
6.712459	621.070574	8.973568
6.554521	612.873336	8.978586
6.797349	618.365840	8.983603
6.785887	621.755333	8.988621
6.560046	623.097404	8.993639
6.994985	624.235568	8.998656
6.751512	625.532531	9.003674
6.690332	621.100495	9.008691
7.069899	636.048828	9.013709
7.042899	629.528598	9.018727
6.915583	615.712902	9.023744
6.761220	619.620118	9.028762
6.911847	617.309548	9.033779
6.646645	615.211925	9.038797
6.482996	616.941306	9.043815
6.765455	635.342484	9.048832
6.891835	652.567646	9.053850
7.265517	644.892941	9.058867
6.882824	647.820330	9.063885
6.814005	641.902058	9.068903
7.185481	630.879729	9.073920
6.691578	633.461581	9.078938
6.937465	625.080738	9.083955
6.903656	642.258799	9.088973
6.950174	635.531916	9.093991
6.914468	637.423564	9.099008
6.678909	642.021350	9.104026
7.123193	638.557303	9.109043
6.705358	644.397199	9.114061
6.875854	642.564994	9.119079
7.083177	637.501719	9.124096
6.963830	649.521479	9.129114
7.145861	646.780537	9.134131
6.766978	646.484486	9.139149
7.056061	650.388939	9.144167
7.077612	652.182136	9.149184
6.984957	655.300456	9.154202
7.378854	638.661015	9.159219
7.141471	654.622691	9.164237
7.138200	628.078263	9.169255
6.958962	618.065582	9.174272
6.740014	627.759269	9.179290
6.731294	632.728121	9.184307
7.161603	639.288327	9.189325
7.302256	647.630637	9.194343
7.414453	649.389730	9.199360
7.076399	636.929885	9.204378
7.338739	618.275780	9.209395
6.686071	622.156863	9.214413
7.008696	624.939299	9.219431
7.268687	632.144593	9.224448
6.995555	642.060239	9.229466
7.018373	639.384834	9.234483
6.921484	646.369727	9.239501
7.115378	644.131117	9.244519
7.523663	652.523590	9.249536
7.286519	639.131151	9.254554
7.175216	623.991235	9.259571
6.830768	618.989223	9.264589
7.126178	634.335323	9.269607
7.402134	633.280285	9.274624
7.314756	639.871895	9.279642
7.170950	623.960643	9.284659
7.192285	616.841510	9.289677
6.936311	614.141614	9.294695
7.210778	622.670003	9.299712
7.034046	641.036412	9.304730
7.274845	638.136734	9.309747
7.153691	645.249258	9.314765
7.200011	646.786992	9.319783
7.018222	640.319750	9.324800
7.126928	646.412585	9.329818
7.523406	645.615522	9.334835
7.375623	641.783017	9.339853
7.058252	642.586152	9.344871
7.420883	639.231879	9.349888
7.101052	644.399882	9.354906
7.327230	636.890741	9.359923
7.339535	639.630677	9.364941
7.051876	647.345539	9.369959
7.458669	636.334089	9.374976
7.244627	638.594222	9.379994
7.322898	639.828654	9.385011
7.374906	639.437627	9.390029
7.182772	651.512352	9.395047
7.230592	644.405749	9.400064
7.002656	646.691804	9.405082
7.165397	643.548770	9.410099
7.063194	649.983992	9.415117
6.972193	649.638496	9.420135
7.224948	644.870233	9.425152
6.982293	644.608508	9.430170
6.723266	642.074456	9.435187
7.143088	658.153467	9.440205
7.266249	674.520189	9.445223
7.335830	664.389310	9.450240
7.411009	676.042254	9.455258
7.310952	679.224596	9.460275
7.678350	675.974440	9.465293
7.457220	677.504896	9.470311
7.591047	677.393212	9.475328
7.464442	680.976577	9.480346
7.337354	683.062288	9.485363
7.276325	675.854806	9.490381
7.380605	674.954368	9.495399
7.545121	678.361382	9.500416
7.357148	679.671007	9.505434
7.433726	682.513883	9.510451
7.620987	684.272162	9.515469
7.488581	686.768963	9.520487
7.520430	675.507787	9.525504
7.569892	685.984171	9.530522
7.551101	681.044738	9.535539
7.736320	680.163571	9.540557
7.558175	682.191402	9.545575
7.339373	676.372359	9.550592
7.533463	682.439454	9.555610
7.508074	674.433604	9.560627
7.488735	673.509153	9.565645
7.121854	687.840647	9.570663
7.784744	683.846524	9.575680
7.606123	684.365874	9.580698
7.345177	676.135270	9.585715
7.467090	677.828391	9.590733
7.425563	685.991849	9.595751
7.548131	678.408316	9.600768
7.398665	685.727108	9.605786
7.585788	681.005134	9.610803
7.736984	683.567757	9.615821
7.472104	678.749584	9.620839
7.886722	669.264272	9.625856
7.592164	679.784040	9.630874
7.663938	679.074602	9.635891
7.990584	673.855344	9.640909
7.739146	683.076721	9.645927
7.398596	680.768747	9.650944
7.559418	691.684340	9.655962
7.261411	690.546209	9.660979
7.871206	674.292210	9.665997
7.587923	684.294006	9.671015
7.604373	677.249272	9.676032
7.648484	682.134592	9.681050
7.422596	687.688207	9.686067
7.800267	680.662191	9.691085
7.441642	681.209972	9.696103
7.569641	688.973336	9.701120
7.864033	696.942598	9.706138
7.852933	690.862002	9.711155
7.874554	691.274772	9.716173
7.496117	685.840995	9.721191
7.821378	690.365607	9.726208
7.884836	691.423570	9.731226
7.615335	691.376513	9.736243
7.586060	700.727635	9.741261
7.578776	708.298268	9.746279
7.986719	707.335140	9.751296
7.966812	708.545484	9.756314
8.049192	711.518695	9.761331
8.363518	707.127199	9.766349
7.740385	692.056229	9.771367
7.689533	690.135880	9.776384
7.561003	685.485269	9.781402
7.447758	696.542898	9.786419
7.902923	702.082744	9.791437
7.662928	715.311433	9.796455
7.664946	702.415913	9.801472
7.792249	706.455629	9.806490
7.804571	713.949598	9.811507
8.449359	711.898497	9.816525
8.054729	704.873797	9.821543
8.111923	704.590761	9.826560
7.746877	708.176219	9.831578
7.592519	710.483168	9.836595
8.104746	705.388078	9.841613
7.680973	707.477060	9.846631
7.975067	714.942477	9.851648
7.992294	706.721692	9.856666
7.848647	710.957844	9.861683
7.743206	703.818920	9.866701
7.903856	720.412342	9.871719
8.165476	715.276471	9.876736
7.974816	716.514699	9.881754
8.047891	713.833124	9.886771
8.125373	713.712858	9.891789
7.927397	712.019417	9.896807
8.173401	707.606166	9.901824
7.993975	709.662952	9.906842
7.829434	719.115221	9.911859
8.107222	706.686201	9.916877
8.065195	714.649770	9.921895
8.473089	713.126057	9.926912
8.069911	715.228951	9.931930
7.915140	714.657022	9.936947
8.048147	711.965522	9.941965
7.882973	717.914973	9.946983
7.982106	708.248433	9.952000
8.134707	711.869027	9.957018
7.603278	717.781104	9.962035
8.145584	698.970704	9.967053
7.847805	714.051557	9.972071
8.136518	714.697834	9.977088
8.238138	712.094205	9.982106
8.032247	712.197233	9.987123
8.136599	715.329000	9.992141
8.105457	717.633654	9.997159
8.091445	710.867160	10.002176
8.305222	709.407087	10.007194
8.162798	714.339842	10.012211
8.287808	705.287876	10.017229
8.178288	713.886597	10.022247
7.887721	714.216232	10.027264
8.091245	707.902266	10.032282
8.072128	729.259608	10.037299
8.388139	729.324237	10.042317
8.200049	743.234861	10.047335
8.145859	745.096907	10.052352
8.099402	738.747559	10.057370
8.151121	751.220141	10.062387
8.377800	742.318236	10.067405
8.285215	752.337706	10.072423
8.484128	741.222034	10.077440
8.596644	739.312614	10.082458
8.397923	734.287220	10.087475
8.451162	718.014128	10.092493
8.118272	724.168902	10.097511
8.243922	718.926421	10.102528
8.436489	718.062735	10.107546
7.794178	730.775421	10.112563
8.468396	732.557783	10.117581
8.655201	746.798429	10.122599
8.064031	738.092589	10.127616
8.569118	745.411275	10.132634
8.288580	751.253079	10.137651
8.532309	751.881219	10.142669
8.301520	741.920102	10.147687
8.551843	737.016789	10.152704
8.377278	725.973999	10.157722
8.614483	731.390315	10.162739
8.240677	715.113934	10.167757
8.240535	726.200292	10.172775
8.109729	742.201295	10.177792
8.400224	751.616021	10.182810
8.368879	755.820203	10.187827
8.443716	744.416433	10.192845
8.565118	750.389300	10.197863
8.361984	756.191124	10.202880
8.750368	747.589976	10.207898
8.192156	756.806691	10.212915
8.442915	745.508425	10.217933
8.418712	758.643151	10.222951
8.200150	745.131015	10.227968
8.362092	745.749472	10.232986
8.212916	754.539810	10.238003
8.607258	748.698921	10.243021
8.227150	742.926445	10.248039
8.614652	754.778105	10.253056
8.820178	754.988188	10.258074
8.468881	747.297278	10.263091
8.423965	745.302912	10.268109
8.487565	755.066613	10.273127
8.372741	744.941024	10.278144
8.593212	739.391120	10.283162
8.407850	741.203239	10.288179
8.711756	755.786683	10.293197
8.658046	760.744523	10.298215
8.825613	756.026945	10.303232
8.911232	753.774362	10.308250
8.524127	747.770774	10.313267
8.611690	748.944427	10.318285
8.584231	747.579414	10.323303
8.447489	749.635042	10.328320
8.848745	749.567845	10.333338
8.645750	763.440801	10.338355
8.858298	748.552625	10.343373
8.777600	754.259768	10.348391
8.542937	748.576189	10.353408
8.703963	757.909610	10.358426
8.612319	754.714788	10.363443
8.835141	753.250851	10.368461
8.904530	755.836876	10.373479
8.897703	749.971875	10.378496
8.828027	749.811416	10.383514
8.861747	757.696719	10.388531
8.668468	740.921153	10.393549
8.509568	752.974313	10.398567
8.493374	760.983231	10.403584
9.011414	768.430484	10.408602
8.914749	779.533652	10.413619
8.910819	762.590100	10.418637
8.639547	755.984686	10.423655
8.630227	770.781421	10.428672
8.914069	775.624709	10.433690
8.657399	779.071771	10.438707
8.713794	779.999423	10.443725
8.784098	782.791193	10.448743
8.639761	785.524421	10.453760
9.209832	781.039769	10.458778
8.509281	789.919860	10.463795
9.142307	777.976805	10.468813
9.092674	786.314877	10.473831
8.791917	789.658619	10.478848
9.112367	781.723387	10.483866
8.786980	782.881181	10.488883
9.022292	783.200892	10.493901
9.202366	783.108123	10.498919
8.917477	785.345365	10.503936
9.077036	778.743393	10.508954
9.007640	784.530954	10.513971
9.471934	775.925881	10.518989
9.304165	765.099247	10.524007
8.820645	766.594231	10.529024
9.091980	753.430855	10.534042
9.023136	760.292658	10.539059
8.590294	748.082462	10.544077
9.044996	766.115923	10.549095
8.827066	779.681149	10.554112
8.935714	773.119105	10.559130
8.896077	776.187333	10.564147
9.272485	779.682304	10.569165
9.094348	778.509947	10.574183
9.074874	790.851839	10.579200
9.283811	784.940465	10.584218
9.067298	790.940962	10.589235
8.950514	785.695301	10.594253
9.399443	776.477849	10.599271
8.770788	778.051196	10.604288
9.361507	774.139863	10.609306
9.205874	785.385469	10.614323
9.292878	782.626384	10.619341
9.365039	774.322849	10.624359
8.923593	787.253877	10.629376
9.018571	781.652697	10.634394
9.217139	784.760609	10.639411
9.153586	786.472645	10.644429
8.990652	775.010202	10.649447
8.895881	778.146612	10.654464
8.739571	781.815623	10.659482
8.923763	778.670388	10.664499
8.674104	785.830633	10.669517
9.055473	794.550456	10.674535
8.910330	811.565262	10.679552
9.172292	805.913193	10.684570
8.901627	813.680044	10.689587
9.291557	812.934054	10.694605
9.421303	816.459645	10.699623
9.288803	822.282471	10.704640
9.553914	811.860864	10.709658
9.285311	822.236280	10.714675
9.282433	824.405568	10.719693
9.363289	817.581194	10.724711
9.305383	815.835019	10.729728
9.546227	816.056576	10.734746
9.351590	818.540280	10.739763
9.207149	817.606026	10.744781
9.293976	822.125283	10.749799
8.986165	829.783339	10.754816
9.358951	817.739264	10.759834
9.640805	810.939871	10.764851
9.311602	816.920459	10.769869
9.528367	817.307018	10.774887
9.525508	824.864575	10.779904
9.515655	812.115409	10.784922
9.524760	815.244073	10.789939
9.350345	818.627525	10.794957
9.502666	818.532659	10.799975
9.211913	821.689722	10.804992
9.587070	817.523148	10.810010
9.609324	817.614378	10.815027
9.551451	822.826850	10.820045
9.722193	817.441050	10.825063
9.578728	823.629845	10.830080
9.464914	817.069978	10.835098
9.179024	821.141144	10.840115
9.395494	818.789721	10.845133
9.533429	816.598540	10.850151
9.565281	823.173239	10.855168
9.759971	815.909959	10.860186
9.637321	816.365324	10.865203
9.417240	822.036915	10.870221
9.843822	818.008273	10.875239
9.194934	820.606963	10.880256
9.388808	816.808185	10.885274
9.130959	825.545304	10.890291
9.201948	826.344564	10.895309
9.336321	821.266343	10.900327
9.268019	834.953287	10.905344
9.827146	841.319030	10.910362
9.856146	844.250321	10.915379
9.584930	847.115982	10.920397
9.848929	841.883618	10.925415
9.715589	851.526852	10.930432
9.730417	842.481242	10.935450
9.616981	848.727669	10.940467
9.756855	844.236685	10.945485
9.876152	842.886335	10.950503
9.788835	843.011064	10.955520
9.675754	849.995186	10.960538
9.878712	836.257664	10.965555
9.403661	842.121477	10.970573
9.703366	838.223677	10.975591
9.611636	838.025139	10.980608
9.909512	841.039456	10.985626
9.726575	836.946008	10.990643
9.584441	845.896639	10.995661
9.755543	838.691583	11.000679
9.510009	840.555802	11.005696
9.970535	835.751105	11.010714
9.864827	841.440376	11.015731
10.014452	843.838335	11.020749
9.970861	832.189167	11.025767
9.509797	833.426516	11.030784
9.680667	829.759096	11.035802
9.587443	836.603712	11.040819
9.581151	837.255543	11.045837
10.105196	827.007175	11.050855
9.620510	836.637721	11.055872
9.537469	835.381111	11.060890
9.601770	851.410150	11.065907
9.625001	865.950812	11.070925
10.214889	863.304487	11.075943
10.147345	872.973844	11.080960
10.030498	878.337037	11.085978
10.141469	878.770250	11.090995
9.867008	877.630765	11.096013
10.257803	868.568940	11.101031
10.136095	874.286855	11.106048
10.115640	865.495486	11.111066
10.085121	857.615581	11.116083
9.907291	863.305780	11.121101
10.132030	860.531745	11.126119
9.907414	867.975266	11.131136
10.115737	870.959539	11.136154
10.335971	868.003976	11.141171
9.719774	868.218256	11.146189
10.378616	865.911673	11.151207
10.225839	877.287968	11.156224
10.265518	854.800387	11.161242
10.207006	844.096148	11.166259
10.011091	833.540254	11.171277
10.334854	832.696566	11.176295
9.909691	841.979875	11.181312
10.138223	840.150438	11.186330
10.320622	836.536617	11.191347
9.757547	846.741141	11.196365
10.005181	849.420098	11.201383
10.266674	865.827891	11.206400
10.146151	864.653073	11.211418
10.482017	864.586469	11.216435
10.018366	877.706672	11.221453
9.961996	860.250859	11.226471
10.171599	877.225100	11.231488
10.320573	878.061840	11.236506
10.388325	878.669130	11.241523
10.022346	879.518709	11.246541
10.433858	878.253422	11.251559
10.232957	880.987372	11.256576
10.255900	879.077809	11.261594
10.322043	874.476199	11.266611
10.197214	874.728787	11.271629
10.193287	867.337753	11.276647
10.376692	874.625525	11.281664
10.095879	875.144482	11.286682
10.197633	869.153981	11.291699
10.338676	874.361087	11.296717
10.561679	866.572651	11.301735
10.365556	877.995886	11.306752
10.520239	870.818730	11.311770
10.504765	867.223497	11.316787
10.209772	870.749362	11.321805
10.356532	869.842075	11.326823
10.202446	880.333991	11.331840
10.434826	878.727916	11.336858
10.486764	865.383861	11.341875
10.471655	872.386019	11.346893
10.537971	867.203705	11.351911
10.292871	866.179037	11.356928
10.304711	872.810218	11.361946
10.331059	886.131158	11.366963
10.502745	891.742228	11.371981
10.781044	897.341157	11.376999
10.709252	896.243695	11.382016
10.789493	891.308266	11.387034
10.854198	875.506313	11.392051
10.355071	864.321907	11.397069
10.626916	865.999669	11.402087
10.641419	871.463542	11.407104
10.280276	874.542514	11.412122
10.362348	870.974825	11.417139
10.487675	895.215797	11.422157
10.460875	890.302031	11.427175
10.533111	899.726222	11.432192
10.609672	906.419530	11.437210
10.538212	895.898886	11.442227
10.367364	905.982988	11.447245
10.538965	906.304985	11.452263
10.450179	901.645956	11.457280
10.516543	908.816913	11.462298
10.814672	903.805243	11.467315
10.673753	896.895519	11.472333
10.469549	896.030603	11.477351
10.614849	902.433407	11.482368
10.501782	901.430176	11.487386
10.726942	902.481061	11.492403
10.477729	902.271595	11.497421
10.568531	923.707454	11.502439
11.004041	930.367312	11.507456
11.036834	927.552221	11.512474
10.808249	918.388617	11.517491
10.731704	917.164388	11.522509
10.666937	918.167227	11.527527
10.875367	926.406736	11.532544
10.728926	939.013460	11.537562
10.904091	934.574871	11.542579
10.718791	937.245620	11.547597
10.804566	940.809622	11.552615
10.832523	935.128545	11.557632
10.812650	937.560886	11.562650
10.985283	935.045848	11.567667
10.689718	938.482458	11.572685
10.583627	935.193146	11.577703
10.924810	931.851024	11.582720
10.846392	935.694564	11.587738
11.073953	932.151584	11.592755
11.077534	938.234582	11.597773
11.090153	938.587632	11.602791
11.255826	929.096934	11.607808
10.927389	939.965777	11.612826
11.021175	933.304557	11.617843
11.143134	938.754990	11.622861
11.121891	934.661115	11.627879
11.132993	931.578763	11.632896
10.959816	940.092879	11.637914
11.471017	922.550880	11.642931
11.216606	943.595531	11.647949
10.948158	938.440286	11.652967
11.016581	933.251302	11.657984
10.959039	940.828600	11.663002
11.482819	935.450041	11.668019
11.318641	947.531783	11.673037
11.172062	932.950134	11.678055
11.155395	932.117936	11.683072
11.115314	938.725855	11.688090
11.318897	932.008266	11.693107
11.025070	950.651308	11.698125
11.225151	930.123965	11.703143
11.223913	933.633086	11.708160
11.119861	927.572712	11.713178
11.428776	928.520756	11.718195
11.270826	935.626515	11.723213
11.468087	936.258027	11.728231
11.722830	934.541556	11.733248
11.058265	913.094482	11.738266
11.464243	907.474824	11.743283
11.230756	901.914216	11.748301
11.113680	902.206857	11.753319
11.426676	922.777222	11.758336
11.315121	939.872428	11.763354
11.629341	921.632772	11.768371
11.056411	915.222118	11.773389
11.451081	924.186650	11.778407
11.654485	917.423036	11.783424
11.487019	913.142369	11.788442
11.412532	899.242085	11.793459
11.395007	907.993780	11.798477
11.292064	907.579393	11.803495
11.208600	905.051654	11.808512
11.076158	917.156856	11.813530
11.476081	923.897011	11.818547
11.340519	927.347277	11.823565
11.470265	935.017173	11.828583
11.798562	939.414197	11.833600
11.129802	940.569812	11.838618
11.375161	929.814012	11.843635
11.542772	937.458742	11.848653
11.751234	932.907164	11.853671
11.504546	938.746188	11.858688
11.687506	943.206649	11.863706
11.831591	935.203307	11.868723
11.354804	931.902158	11.873741
11.704352	939.782101	11.878759
11.540844	938.423853	11.883776
11.474998	934.370828	11.888794
11.585796	924.553016	11.893811
11.523654	934.003418	11.898829
11.517207	933.296293	11.903847
11.734824	927.936549	11.908864
11.680385	942.917683	11.913882
11.916302	937.230118	11.918899
11.649173	933.897399	11.923917
11.448856	936.699762	11.928935
11.661617	932.644298	11.933952
11.502503	936.416167	11.938970
11.638451	923.220346	11.943987
11.771904	934.512671	11.949005
11.647805	934.931272	11.954023
11.603601	926.122543	11.959040
11.571675	935.028993	11.964058
11.209239	931.780951	11.969075
11.454613	931.834446	11.974093
11.504173	930.376351	11.979111
11.849693	925.244233	11.984128
11.607902	937.680929	11.989146
11.657851	953.793942	11.994163
11.961279	953.181163	11.999181
12.019038	958.098167	12.004199
11.931640	959.935818	12.009216
11.401793	958.336281	12.014234
11.746356	955.611281	12.019251
12.135523	962.721326	12.024269
11.809645	963.657572	12.029287
12.144450	973.167847	12.034304
12.073151	959.853566	12.039322
12.357157	948.207538	12.044339
12.455184	943.724637	12.049357
11.718140	933.962975	12.054375
11.934439	931.237961	12.059392
11.756159	935.694071	12.064410
12.190299	927.869066	12.069427
11.801826	929.980576	12.074445
11.670633	928.403997	12.079463
11.992794	953.249440	12.084480
12.094082	953.063029	12.089498
11.773832	959.489017	12.094515
12.142683	966.160324	12.099533
12.113381	965.357381	12.104551
12.018693	965.497110	12.109568
11.849751	961.221398	12.114586
12.142628	965.444776	12.119603
12.111163	962.821020	12.124621
11.881726	965.777416	12.129639
12.389968	958.776698	12.134656
12.203911	958.130809	12.139674
12.032389	959.037556	12.144691
12.138431	959.614887	12.149709
12.327668	959.661538	12.154727
12.356933	956.776950	12.159744
12.314741	958.618138	12.164762
12.353424	965.039411	12.169779
12.022580	960.436591	12.174797
12.204035	971.000162	12.179815
12.289425	968.778687	12.184832
12.357834	970.621245	12.189850
12.209648	966.755460	12.194867
12.121484	972.302510	12.199885
12.092719	964.951368	12.204903
12.310502	956.474022	12.209920
12.203901	969.247787	12.214938
12.265447	964.603212	12.219955
12.481339	965.682013	12.224973
12.032826	972.424114	12.229991
12.504030	967.380219	12.235008
12.040431	967.351130	12.240026
12.143879	958.795083	12.245043
12.056294	961.236280	12.250061
11.966112	972.071989	12.255079
12.570311	982.481314	12.260096
12.793755	989.958170	12.265114
12.665917	990.624624	12.270131
12.513813	975.173419	12.275149
12.180258	978.819075	12.280167
12.418581	975.858133	12.285184
12.362438	995.333087	12.290202
12.626548	994.081178	12.295219
12.604854	994.811941	12.300237
12.275773	1001.554748	12.305255
12.438075	993.349943	12.310272
11.958130	991.963388	12.315290
12.203346	992.576726	12.320307
12.569709	994.097518	12.325325
12.407556	996.738855	12.330343
12.584521	997.221376	12.335360
12.779495	1001.638527	12.340378
12.566180	998.964174	12.345395
12.719834	993.030381	12.350413
12.798439	1002.683097	12.355431
12.728217	999.842141	12.360448
12.563512	1003.481493	12.365466
12.765878	1000.523746	12.370483
12.722910	986.974052	12.375501
12.401773	995.060754	12.380519
12.626735	997.052185	12.385536
12.463684	1000.734568	12.390554
12.522999	1001.701117	12.395571
12.626526	1008.317960	12.400589
12.715394	1030.137733	12.405607
12.918823	1030.346986	12.410624
13.177369	1032.429707	12.415642
12.790902	1018.754200	12.420659
13.036162	1016.434593	12.425677
12.838320	1005.926143	12.430695
12.729163	1003.456971	12.435712
12.581897	1004.250653	12.440730
12.867510	1021.074675	12.445747
12.909639	1021.955493	12.450765
12.784158	1023.512070	12.455783
12.724255	1029.568217	12.460800
12.752644	1035.019219	12.465818
12.668609	1035.904396	12.470835
12.941343	1031.143336	12.475853
12.592186	1037.719019	12.480871
12.906370	1025.271908	12.485888
13.013735	1030.853919	12.490906
12.742177	1031.361900	12.495923
12.904976	1028.139058	12.500941
12.651994	1025.988962	12.505959
12.851563	1026.311842	12.510976
12.792659	1028.943567	12.515994
12.832826	1045.540557	12.521011
13.065172	1056.735889	12.526029
12.649725	1066.579509	12.531047
12.988357	1062.966928	12.536064
13.176787	1071.566503	12.541082
13.113928	1064.897704	12.546099
13.438519	1065.038471	12.551117
13.016067	1061.281858	12.556135
13.112579	1062.280045	12.561152
13.019255	1067.361467	12.566170
13.001523	1066.231419	12.571187
13.383894	1056.883097	12.576205
13.462062	1068.470883	12.581223
13.511772	1058.185171	12.586240
13.274548	1062.105039	12.591258
13.230239	1055.365851	12.596275
13.461641	1060.026189	12.601293
13.314795	1062.094161	12.606311
13.608344	1063.391200	12.611328
13.397452	1061.504197	12.616346
13.186931	1059.054952	12.621363
13.388933	1062.383996	12.626381
12.996862	1067.392454	12.631399
13.228437	1066.056168	12.636416
13.799593	1062.501139	12.641434
13.374650	1064.428557	12.646451
13.547172	1054.758703	12.651469
13.197852	1065.083871	12.656487
13.135879	1055.161129	12.661504
13.687596	1056.525254	12.666522
13.524427	1059.430144	12.671539
13.433837	1057.501960	12.676557
13.385222	1061.746484	12.681575
13.487821	1064.991600	12.686592
13.371216	1060.426497	12.691610
13.348361	1061.323590	12.696627
13.508530	1056.989808	12.701645
13.256916	1062.641906	12.706663
13.606296	1057.720515	12.711680
13.659809	1055.053931	12.716698
13.437428	1068.980367	12.721715
13.604345	1058.883504	12.726733
13.533937	1058.235782	12.731751
13.576020	1058.230427	12.736768
13.297764	1057.097855	12.741786
13.421986	1055.617149	12.746803
13.641183	1056.787137	12.751821
13.268575	1063.528124	12.756839
13.314316	1054.476878	12.761856
13.462746	1073.983405	12.766874
13.341149	1090.680063	12.771891
13.890068	1086.090564	12.776909
13.811693	1090.505766	12.781927
13.637206	1095.265218	12.786944
14.143523	1102.339787	12.791962
13.748578	1098.638450	12.796979
13.926501	1101.812835	12.801997
13.813192	1095.757470	12.807015
13.527339	1086.700096	12.812032
13.426849	1090.532763	12.817050
13.446258	1093.024763	12.822067
13.693508	1092.152396	12.827085
13.797300	1099.006231	12.832103
14.171402	1094.222854	12.837120
14.221561	1096.638112	12.842138
13.945948	1094.365382	12.847155
14.102453	1093.035225	12.852173
14.054895	1092.810866	12.857191
13.925107	1099.936444	12.862208
14.093413	1087.416201	12.867226
13.690788	1101.086699	12.872243
14.043370	1095.137247	12.877261
14.020787	1092.118313	12.882279
13.955052	1093.310292	12.887296
14.143679	1088.870218	12.892314
13.873775	1093.559647	12.897331
14.138288	1089.469590	12.902349
13.819221	1087.407985	12.907367
13.838047	1084.728637	12.912384
14.041445	1087.854708	12.917402
13.856975	1092.447315	12.922419
14.089702	1095.102407	12.927437
14.253347	1091.237706	12.932455
13.884140	1086.451444	12.937472
13.947231	1090.936523	12.942490
14.052796	1096.061000	12.947507
14.015231	1091.209581	12.952525
14.283166	1096.271737	12.957543
14.155746	1094.711445	12.962560
14.382996	1092.602675	12.967578
14.387893	1090.637415	12.972595
14.306203	1089.242378	12.977613
14.211051	1097.093292	12.982631
14.204864	1091.213095	12.987648
14.157111	1086.824764	12.992666
14.333747	1090.039121	12.997683
14.255927	1083.097606	13.002701
14.314739	1094.385873	13.007719
14.014832	1085.912299	13.012736
14.409655	1091.152253	13.017754
14.198462	1102.462405	13.022771
14.570446	1099.616308	13.027789
14.194566	1102.390690	13.032807
14.181078	1109.166317	13.037824
14.157680	1113.435419	13.042842
14.215158	1124.195603	13.047859
14.326203	1127.070056	13.052877
14.484882	1124.356912	13.057895
14.045196	1127.911914	13.062912
14.598145	1119.767937	13.067930
14.278460	1123.101105	13.072947
14.604249	1124.617212	13.077965
14.558779	1116.767997	13.082983
14.500629	1125.584414	13.088000
14.609326	1113.856668	13.093018
14.388436	1124.885776	13.098035
14.717839	1117.102035	13.103053
14.188698	1130.349039	13.108071
14.040754	1130.255865	13.113088
14.544667	1134.919915	13.118106
14.463545	1153.054372	13.123123
14.708896	1156.336101	13.128141
14.826096	1155.619513	13.133159
14.125757	1149.168051	13.138176
14.879796	1148.885353	13.143194
14.533461	1154.683481	13.148211
14.782807	1146.177577	13.153229
14.854059	1153.908447	13.158247
14.806792	1153.561602	13.163264
14.911605	1151.223109	13.168282
14.643123	1159.173621	13.173299
14.663797	1146.047092	13.178317
14.502676	1158.910353	13.183335
14.425891	1146.259790	13.188352
14.692595	1149.364760	13.193370
14.122845	1144.811682	13.198387
14.435922	1155.710263	13.203405
14.715683	1169.617805	13.208423
14.558839	1187.469576	13.213440
14.690850	1179.923604	13.218458
14.891020	1193.358931	13.223475
15.095258	1183.106600	13.228493
15.069529	1180.075178	13.233511
15.279144	1193.218400	13.238528
14.906139	1189.086256	13.243546
14.989452	1196.065963	13.248563
15.379158	1188.354482	13.253581
15.024257	1191.518305	13.258599
14.869046	1197.017484	13.263616
15.177458	1191.411914	13.268634
14.769116	1193.031096	13.273651
15.095677	1196.883224	13.278669
15.402950	1188.541715	13.283687
15.164617	1194.775500	13.288704
15.103432	1184.932070	13.293722
15.025640	1194.515531	13.298739
15.257262	1194.386272	13.303757
15.231476	1186.660923	13.308775
15.199114	1193.042482	13.313792
15.295658	1178.064055	13.318810
15.271431	1188.367357	13.323827
14.752407	1186.601048	13.328845
14.848143	1193.554681	13.333863
14.896293	1192.005066	13.338880
15.567839	1185.455535	13.343898
15.555312	1192.369224	13.348915
15.232183	1184.031327	13.353933
15.384865	1191.362130	13.358951
15.247959	1191.747427	13.363968
15.374024	1185.246889	13.368986
15.478129	1188.123684	13.374003
15.282418	1198.276657	13.379021
15.440483	1195.539588	13.384039
15.280849	1204.237033	13.389056
15.412851	1199.253172	13.394074
15.474879	1200.570848	13.399091
15.115806	1198.267436	13.404109
15.446214	1183.867184	13.409127
15.481788	1200.097003	13.414144
15.221416	1192.252629	13.419162
15.168524	1200.109982	13.424179
15.487343	1210.595853	13.429197
15.797573	1209.881548	13.434215
15.273032	1224.119175	13.439232
15.438495	1219.094336	13.444250
15.617805	1217.939914	13.449267
15.673239	1229.567411	13.454285
16.192969	1223.656764	13.459303
15.375671	1213.444055	13.464320
15.569890	1208.497919	13.469338
15.643357	1212.555738	13.474355
15.663893	1211.745709	13.479373
15.497856	1222.497307	13.484391
15.233507	1223.546209	13.489408
15.511640	1218.895612	13.494426
15.328978	1219.790439	13.499443
15.370440	1223.913401	13.504461
15.662693	1217.623118	13.509479
15.706638	1224.673527	13.514496
15.742939	1219.094111	13.519514
15.698134	1228.398912	13.524531
15.407075	1221.488710	13.529549
15.808282	1238.407208	13.534567
15.928332	1254.719154	13.539584
15.957471	1240.875417	13.544602
15.573862	1239.744924	13.549619
15.826627	1253.459774	13.554637
16.121586	1249.442190	13.559655
16.065915	1255.137498	13.564672
15.861997	1253.511513	13.569690
16.007966	1256.359341	13.574707
16.018708	1255.097009	13.579725
15.964097	1251.858945	13.584743
15.773972	1258.645385	13.589760
16.029354	1257.244118	13.594778
16.129358	1260.600725	13.599795
16.099721	1252.338202	13.604813
16.401432	1253.702409	13.609831
16.209107	1250.758401	13.614848
16.287395	1245.919244	13.619866
16.134692	1234.236664	13.624883
16.078720	1227.326110	13.629901
16.146749	1228.152653	13.634919
16.065521	1239.755545	13.639936
16.255626	1234.035697	13.644954
16.007230	1240.221168	13.649971
16.251151	1249.177390	13.654989
16.529274	1247.411345	13.660007
16.379298	1251.032175	13.665024
16.183997	1234.754819	13.670042
16.315270	1236.293700	13.675059
16.139703	1234.721288	13.680077
16.357338	1230.936979	13.685095
16.307339	1242.374471	13.690112
16.260732	1243.257398	13.695130
16.319317	1245.650812	13.700147
16.042872	1254.192043	13.705165
16.374578	1240.057658	13.710183
16.270403	1249.470331	13.715200
16.463973	1243.278660	13.720218
16.253656	1243.700524	13.725235
16.098239	1253.971266	13.730253
16.147482	1245.031924	13.735271
16.056202	1247.013948	13.740288
16.109429	1242.232090	13.745306
16.425931	1256.867856	13.750323
16.562621	1280.147734	13.755341
16.688808	1269.958269	13.760359
16.535924	1266.195940	13.765376
16.463491	1268.933092	13.770394
16.572808	1281.437899	13.775411
16.704722	1283.279821	13.780429
16.703382	1265.595942	13.785447
16.306401	1273.891404	13.790464
16.606113	1284.656860	13.795482
16.386238	1275.664431	13.800499
16.336637	1282.676422	13.805517
16.400125	1277.642074	13.810535
16.418444	1287.519511	13.815552
16.444510	1282.472461	13.820570
16.200545	1278.440968	13.825587
16.326460	1291.602071	13.830605
17.062107	1296.900219	13.835623
17.002354	1313.240033	13.840640
16.661556	1294.074974	13.845658
16.482094	1296.492069	13.850675
16.647309	1306.819589	13.855693
16.972229	1311.888521	13.860711
17.036548	1308.461070	13.865728
16.764939	1312.859910	13.870746
17.211370	1308.414875	13.875763
16.821156	1313.463261	13.880781
17.136232	1314.332753	13.885799
16.738183	1313.730222	13.890816
17.359695	1311.635659	13.895834
17.339401	1315.341718	13.900851
17.029609	1299.535211	13.905869
17.162953	1282.962442	13.910887
16.799536	1274.810297	13.915904
16.825107	1269.877896	13.920922
17.149520	1289.733493	13.925939
17.418423	1303.852004	13.930957
17.254040	1285.650628	13.935975
17.029272	1280.567559	13.940992
17.034862	1272.136991	13.946010
17.319319	1268.422708	13.951027
17.226679	1275.013883	13.956045
17.623294	1270.221607	13.961063
17.242674	1278.257283	13.966080
17.363138	1273.871750	13.971098
17.253132	1275.870264	13.976115
17.219761	1271.672800	13.981133
17.121641	1260.442565	13.986151
17.152954	1273.570502	13.991168
17.289013	1275.824716	13.996186
17.363468	1272.332998	14.001203
17.287116	1279.096276	14.006221
17.271937	1279.193707	14.011239
17.413959	1275.599069	14.016256
17.448434	1271.511627	14.021274
17.864785	1272.501350	14.026291
17.390760	1267.855613	14.031309
17.653924	1270.597425	14.036327
17.197916	1270.833998	14.041344
17.224124	1271.943444	14.046362
17.747680	1268.208070	14.051379
17.357424	1278.099225	14.056397
17.654167	1272.019193	14.061415
17.205349	1274.423411	14.066432
17.091892	1285.155322	14.071450
17.295711	1298.800760	14.076467
17.337365	1311.553798	14.081485
17.443738	1313.545619	14.086503
17.317569	1303.394379	14.091520
17.469792	1310.150920	14.096538
17.398064	1307.676682	14.101555
17.435692	1305.184336	14.106573
17.410917	1308.352960	14.111591
17.811693	1311.593631	14.116608
17.462996	1325.103824	14.121626
17.922529	1318.014164	14.126643
17.678532	1330.275165	14.131661
17.847728	1330.430645	14.136679
17.589911	1344.515948	14.141696
17.698930	1332.302956	14.146714
17.819030	1330.063083	14.151731
17.527104	1333.064541	14.156749
18.417137	1323.012717	14.161767
17.841675	1334.739649	14.166784
18.062045	1332.867414	14.171802
17.934826	1334.182583	14.176819
17.828154	1339.095442	14.181837
18.202225	1334.373020	14.186855
17.617454	1335.036024	14.191872
17.972092	1340.322087	14.196890
18.416540	1328.372048	14.201907
18.052857	1327.628002	14.206925
18.077293	1335.884419	14.211943
17.868513	1329.513679	14.216960
17.953481	1334.307402	14.221978
18.047637	1331.871436	14.226995
17.919476	1338.118529	14.232013
17.922024	1338.120902	14.237031
17.867617	1338.076803	14.242048
17.626427	1331.429546	14.247066
17.945914	1325.298485	14.252083
17.747708	1336.361386	14.257101
17.835349	1334.874901	14.262119
18.325421	1350.969378	14.267136
18.142626	1360.664423	14.272154
18.319859	1363.935824	14.277171
18.032025	1362.010739	14.282189
18.326540	1359.307737	14.287207
18.195949	1363.184038	14.292224
18.310481	1359.505352	14.297242
18.130433	1358.983251	14.302259
18.425766	1359.502874	14.307277
18.024662	1358.426842	14.312295
18.410979	1366.692638	14.317312
18.463804	1369.849606	14.322330
18.597107	1356.844797	14.327347
18.176411	1362.196664	14.332365
18.529210	1363.579979	14.337383
18.627886	1355.568980	14.342400
18.076554	1368.329714	14.347418
18.644980	1350.456899	14.352435
18.522977	1363.622505	14.357453
18.635552	1359.404393	14.362471
18.641231	1361.990046	14.367488
18.515710	1364.874979	14.372506
18.491050	1350.663684	14.377523
18.420382	1361.557455	14.382541
18.461587	1360.018422	14.387559
18.380509	1357.692572	14.392576
18.786811	1375.822947	14.397594
19.156668	1366.018256	14.402611
18.723652	1371.236736	14.407629
18.753818	1356.793133	14.412647
18.758401	1355.304653	14.417664
18.936529	1354.990161	14.422682
18.785534	1353.779013	14.427699
18.899349	1355.965665	14.432717
18.811854	1355.714845	14.437735
18.829868	1354.267447	14.442752
18.630700	1356.589391	14.447770
18.832553	1375.766198	14.452787
19.235511	1374.112928	14.457805
18.999936	1364.371883	14.462823
19.121831	1355.272419	14.467840
19.159196	1352.223428	14.472858
19.170722	1352.640446	14.477875
18.712476	1349.887697	14.482893
19.205568	1355.358312	14.487911
18.978718	1349.602747	14.492928
18.783295	1353.260259	14.497946
19.149535	1347.024993	14.502963
19.062156	1356.156609	14.507981
18.853035	1355.716486	14.512999
19.091805	1366.111391	14.518016
18.987823	1382.557813	14.523034
19.070747	1382.484672	14.528051
18.890954	1386.991948	14.533069
18.962219	1383.238140	14.538087
19.532918	1375.943829	14.543104
19.185744	1386.503100	14.548122
19.462032	1378.285910	14.553139
19.063088	1388.589194	14.558157
19.340475	1387.309073	14.563175
19.074882	1384.180327	14.568192
19.218038	1386.196773	14.573210
19.300658	1375.114080	14.578227
18.746160	1383.110495	14.583245
18.973627	1386.098391	14.588263
19.192495	1380.768600	14.593280
19.082074	1399.642825	14.598298
19.399800	1408.929430	14.603315
19.600496	1418.709428	14.608333
19.460915	1412.308691	14.613351
19.654355	1414.285319	14.618368
19.369522	1411.631791	14.623386
19.455108	1410.074381	14.628403
19.721281	1417.182958	14.633421
19.632946	1416.293312	14.638439
19.720140	1404.016163	14.643456
19.579605	1412.761742	14.648474
19.574753	1409.320133	14.653491
19.491699	1409.031175	14.658509
19.435969	1415.769838	14.663527
19.663585	1403.241488	14.668544
19.389527	1415.485487	14.673562
19.523831	1407.019358	14.678579
19.601357	1408.115986	14.683597
19.486196	1409.957500	14.688615
19.569758	1403.183601	14.693632
19.770572	1415.651318	14.698650
20.122279	1412.322313	14.703667
19.814165	1414.993402	14.708685
19.486890	1421.208542	14.713703
19.840118	1423.220914	14.718720
19.764024	1432.140474	14.723738
20.508540	1435.174645	14.728755
20.301156	1425.091891	14.733773
20.150722	1409.326991	14.738791
19.973422	1399.860125	14.743808
19.533233	1411.165116	14.748826
19.626043	1408.856131	14.753843
19.686305	1421.773104	14.758861
19.620982	1428.073605	14.763879
20.342915	1429.001318	14.768896
20.066695	1438.784716	14.773914
20.508084	1430.522441	14.778931
20.250362	1432.669450	14.783949
20.059466	1437.429362	14.788967
20.270887	1431.916931	14.793984
20.008904	1428.731280	14.799002
20.158827	1431.009599	14.804019
20.278741	1429.692954	14.809037
20.152483	1436.239766	14.814055
20.374392	1436.819975	14.819072
20.053998	1422.093424	14.824090
20.334858	1422.563479	14.829107
20.488292	1433.860339	14.834125
20.338814	1427.162422	14.839143
20.556047	1428.773701	14.844160
20.429625	1431.745801	14.849178
20.867851	1430.188259	14.854195
20.513344	1433.693397	14.859213
20.481003	1431.439778	14.864231
20.583739	1432.571996	14.869248
20.621519	1433.674026	14.874266
20.465186	1422.704884	14.879283
20.657154	1429.461982	14.884301
20.513771	1435.512426	14.889319
20.839202	1427.393762	14.894336
20.416636	1425.692945	14.899354
20.694510	1423.358429	14.904371
20.532553	1425.371864	14.909389
20.466637	1430.021315	14.914407
20.923117	1426.932826	14.919424
20.631305	1431.982277	14.924442
20.711152	1433.068286	14.929459
20.825532	1422.612571	14.934477
21.039609	1431.874229	14.939495
20.797482	1419.311452	14.944512
20.598058	1414.690275	14.949530
20.869403	1421.612568	14.954547
20.745749	1417.523714	14.959565
20.738150	1425.571315	14.964583
21.090452	1429.309793	14.969600
20.474735	1434.152257	14.974618
20.723950	1426.494238	14.979635
20.959699	1425.222584	14.984653
21.014781	1428.783514	14.989671
21.204846	1424.405309	14.994688
20.800660	1430.219811	14.999706
20.764003	1432.275095	15.004723
20.997021	1425.899657	15.009741
20.933163	1432.846756	15.014759
20.869089	1426.420518	15.019776
20.926118	1427.032361	15.024794
21.044493	1430.913906	15.029811
20.637426	1435.678512	15.034829
20.945521	1444.268322	15.039847
20.834171	1453.714983	15.044864
21.176448	1457.031907	15.049882
21.236513	1456.548385	15.054899
21.183311	1454.358453	15.059917
21.209417	1459.128891	15.064935
21.233044	1459.691544	15.069952
21.330677	1460.591542	15.074970
21.334410	1465.169234	15.079987
21.331038	1462.671447	15.085005
21.153581	1472.238514	15.090023
21.336010	1460.951045	15.095040
21.418313	1460.228018	15.100058
20.973634	1468.770454	15.105075
21.360799	1462.698210	15.110093
21.121568	1462.634717	15.115111
21.392555	1464.683154	15.120128
21.226016	1462.486792	15.125146
20.978878	1482.367994	15.130163
21.366665	1488.415929	15.135181
21.305095	1494.764261	15.140199
21.912908	1491.147951	15.145216
21.631512	1497.300012	15.150234
21.710258	1486.989917	15.155251
21.888341	1493.121792	15.160269
21.513402	1490.622541	15.165287
21.969162	1485.762926	15.170304
22.005903	1492.261903	15.175322
21.777117	1493.892718	15.180339
21.931828	1483.822404	15.185357
21.776191	1494.100821	15.190375
21.555690	1495.285783	15.195392
21.677674	1495.612074	15.200410
21.731427	1492.585539	15.205427
21.983336	1483.398722	15.210445
21.925726	1493.303037	15.215463
22.241987	1484.744530	15.220480
21.939928	1492.254715	15.225498
21.975195	1488.242674	15.230515
22.213607	1488.354805	15.235533
21.974614	1499.715517	15.240551
22.271833	1492.927851	15.245568
22.307076	1484.491470	15.250586
21.789572	1475.291916	15.255603
21.655410	1465.458030	15.260621
21.760385	1488.687963	15.265639
22.165790	1480.152097	15.270656
22.117915	1497.291701	15.275674
21.943325	1489.449506	15.280691
22.131426	1480.721676	15.285709
21.917632	1485.444450	15.290727
22.021284	1479.456549	15.295744
22.051840	1486.087648	15.300762
21.854879	1496.211100	15.305779
22.315308	1491.924324	15.310797
21.946552	1495.986946	15.315815
22.299980	1508.536157	15.320832
22.252102	1517.714475	15.325850
22.111090	1526.861766	15.330867
22.369647	1516.523450	15.335885
21.928771	1518.981506	15.340903
21.837630	1522.022583	15.345920
22.413079	1519.654130	15.350938
22.266078	1524.493018	15.355955
22.344145	1508.204357	15.360973
22.170106	1523.423570	15.365991
22.586744	1531.323808	15.371008
22.732644	1540.339344	15.376026
23.021921	1539.532433	15.381043
23.094610	1519.603748	15.386061
22.457071	1507.795346	15.391079
22.702009	1517.773982	15.396096
22.839551	1513.964286	15.401114
22.666658	1509.923719	15.406131
22.689526	1501.121666	15.411149
22.623793	1508.358475	15.416167
22.527152	1506.670604	15.421184
22.860108	1519.335417	15.426202
22.809900	1539.371086	15.431219
23.089837	1533.281138	15.436237
22.897584	1534.040171	15.441255
22.975013	1530.506170	15.446272
23.174284	1516.006857	15.451290
22.858333	1508.559710	15.456307
23.159735	1499.895783	15.461325
23.005915	1506.145224	15.466343
22.589983	1503.941730	15.471360
22.928691	1513.945781	15.476378
23.089100	1527.422234	15.481395
23.091189	1537.997392	15.486413
23.111331	1544.476699	15.491431
23.254870	1534.766465	15.496448
23.176222	1531.303979	15.501466
23.265441	1533.166387	15.506483
23.444867	1519.741603	15.511501
23.181371	1512.788124	15.516519
23.329890	1509.870694	15.521536
22.888980	1501.224968	15.526554
23.021727	1527.938894	15.531571
23.455425	1522.419938	15.536589
23.601847	1527.777946	15.541607
23.145510	1532.311374	15.546624
23.352098	1536.356682	15.551642
23.165697	1534.619499	15.556659
23.326477	1526.824503	15.561677
23.322095	1532.229533	15.566695
23.480662	1530.018694	15.571712
23.726628	1527.609527	15.576730
23.291544	1536.579933	15.581747
23.375950	1529.484977	15.586765
23.601745	1534.697562	15.591783
23.380761	1527.370899	15.596800
23.702257	1521.717375	15.601818
23.308368	1527.214857	15.606835
23.748867	1532.103308	15.611853
23.436708	1533.563684	15.616871
23.487256	1532.845912	15.621888
23.440144	1529.710877	15.626906
23.384751	1533.069655	15.631923
23.844920	1529.820301	15.636941
23.481762	1538.776830	15.641959
23.292804	1553.341463	15.646976
23.713230	1559.329298	15.651994
23.855467	1562.745512	15.657011
23.922954	1564.080031	15.662029
23.787110	1566.350182	15.667047
23.697105	1575.952830	15.672064
24.363527	1567.344166	15.677082
23.868602	1570.440308	15.682099
23.892101	1566.417990	15.687117
23.853364	1565.567760	15.692135
24.142906	1558.310082	15.697152
23.863382	1558.433967	15.702170
23.759841	1558.596033	15.707187
24.160729	1555.954910	15.712205
23.735416	1561.907996	15.717223
23.894371	1567.395044	15.722240
24.134691	1561.751799	15.727258
24.216880	1571.398763	15.732275
24.099117	1579.089493	15.737293
24.078963	1581.626705	15.742311
24.337850	1593.415663	15.747328
24.491725	1595.446504	15.752346
24.374311	1594.006943	15.757363
24.473691	1588.121282	15.762381
24.447855	1590.028340	15.767399
24.233400	1586.189121	15.772416
24.375429	1586.415638	15.777434
24.178182	1593.463637	15.782451
24.251781	1590.636551	15.787469
24.408060	1591.575663	15.792487
24.205663	1588.902942	15.797504
24.670809	1586.718492	15.802522
24.651328	1593.334694	15.807539
24.452452	1580.548090	15.812557
24.374575	1583.562968	15.817575
24.499500	1590.906037	15.822592
24.737333	1591.582827	15.827610
24.471814	1592.468561	15.832627
24.571094	1591.513585	15.837645
24.630715	1581.828242	15.842663
24.488258	1588.062842	15.847680
24.757730	1594.327261	15.852698
24.530439	1598.467662	15.857715
24.980380	1600.842386	15.862733
24.732198	1602.542960	15.867751
24.668534	1617.795955	15.872768
25.313049	1618.489259	15.877786
24.864196	1611.037693	15.882803
24.569026	1608.738990	15.887821
25.130502	1613.538143	15.892839
25.024336	1615.764016	15.897856
25.457360	1615.098257	15.902874
24.911656	1606.234394	15.907891
25.085349	1601.179329	15.912909
24.835062	1603.839300	15.917927
25.021443	1617.794598	15.922944
24.887810	1619.899037	15.927962
25.071033	1619.840782	15.932979
25.278576	1619.894641	15.937997
25.540955	1615.880391	15.943015
25.418162	1621.313327	15.948032
25.315502	1613.130420	15.953050
25.333608	1624.288807	15.958067
25.428779	1611.080652	15.963085
25.443333	1606.273196	15.968103
25.121890	1620.203931	15.973120
25.480798	1613.309541	15.978138
25.479834	1613.216040	15.983155
25.378550	1616.328893	15.988173
25.353395	1622.301564	15.993191
25.487481	1617.997142	15.998208
25.685561	1613.908501	16.003226
25.485733	1623.910071	16.008243
25.565717	1614.913852	16.013261
25.427465	1612.227354	16.018279
25.688379	1613.937718	16.023296
25.800548	1616.395151	16.028314
25.574603	1614.670412	16.033331
25.862143	1608.218549	16.038349
25.632199	1607.135808	16.043367
25.434229	1616.232741	16.048384
25.630791	1608.072727	16.053402
25.746664	1620.848768	16.058419
25.799344	1608.297647	16.063437
25.929573	1612.386329	16.068455
25.404549	1622.527575	16.073472
25.917846	1606.336423	16.078490
25.736000	1613.944475	16.083507
26.016196	1611.928443	16.088525
25.869286	1611.845330	16.093543
25.659336	1617.747026	16.098560
25.917459	1607.755570	16.103578
25.638658	1612.515130	16.108595
26.082125	1626.934554	16.113613
26.292743	1638.579179	16.118631
25.730325	1647.071131	16.123648
25.996864	1632.612538	16.128666
26.138649	1641.812278	16.133683
25.724405	1648.193090	16.138701
26.281420	1651.152844	16.143719
25.822746	1641.690693	16.148736
26.201457	1642.391007	16.153754
26.303976	1643.858708	16.158771
26.174398	1641.092029	16.163789
26.283552	1652.260162	16.168807
26.342427	1646.254021	16.173824
26.511614	1642.613463	16.178842
26.320390	1651.046704	16.183859
26.347152	1648.133663	16.188877
26.254233	1639.209762	16.193895
26.318296	1642.547601	16.198912
26.526322	1661.624921	16.203930
26.577625	1671.870761	16.208947
26.731098	1664.319819	16.213965
26.974411	1655.422513	16.218983
26.669998	1645.776942	16.224000
26.719818	1642.339219	16.229018
26.815037	1630.014894	16.234035
26.667739	1636.253464	16.239053
26.274480	1640.467424	16.244071
26.348695	1649.452768	16.249088
26.831335	1659.961423	16.254106
26.935152	1669.020223	16.259123
26.658064	1665.127971	16.264141
26.892876	1663.376534	16.269159
26.611906	1662.497513	16.274176
26.892901	1668.195489	16.279194
26.972741	1663.561457	16.284211
26.900152	1666.208940	16.289229
27.010904	1656.795398	16.294247
27.239347	1658.322168	16.299264
27.149074	1660.363133	16.304282
27.146684	1660.836401	16.309299
26.863521	1665.510873	16.314317
27.022618	1655.173188	16.319335
27.301218	1657.810152	16.324352
27.387491	1652.349863	16.329370
27.304644	1657.158090	16.334387
27.051252	1656.870958	16.339405
27.262995	1656.298927	16.344423
27.310170	1655.913203	16.349440
27.318142	1646.103303	16.354458
27.440176	1649.547685	16.359475
27.241004	1657.277131	16.364493
27.320977	1655.626532	16.369511
27.234365	1662.635375	16.374528
27.265334	1652.074028	16.379546
27.297183	1656.428617	16.384563
27.241320	1648.072982	16.389581
27.594009	1651.245312	16.394599
27.350478	1649.716788	16.399616
27.507233	1649.300713	16.404634
27.552991	1661.256906	16.409651
27.508219	1674.011562	16.414669
27.680918	1681.938888	16.419687
27.877602	1688.890594	16.424704
27.828479	1685.614522	16.429722
27.804196	1685.168189	16.434739
27.758154	1688.057737	16.439757
27.904163	1681.302510	16.444775
27.787353	1680.855358	16.449792
28.064595	1682.046491	16.454810
27.862243	1678.343828	16.459827
27.616875	1671.312865	16.464845
27.836334	1680.081263	16.469863
27.905830	1687.614265	16.474880
27.843271	1683.349476	16.479898
27.681314	1681.528308	16.484915
27.819770	1683.986516	16.489933
27.774291	1682.519286	16.494951
27.638242	1686.051296	16.499968
28.096958	1681.197037	16.504986
28.060036	1670.905187	16.510003
28.171503	1676.659979	16.515021
28.243665	1665.816212	16.520039
28.174280	1679.858802	16.525056
28.105445	1691.793050	16.530074
28.415831	1703.942068	16.535091
28.487867	1706.673089	16.540109
28.022614	1684.547449	16.545127
28.035750	1699.094107	16.550144
28.565335	1705.711560	16.555162
28.671660	1710.016824	16.560179
28.577439	1713.258842	16.565197
28.657494	1700.970436	16.570215
28.772668	1696.966762	16.575232
28.497448	1683.547834	16.580250
28.383286	1676.538055	16.585267
28.160116	1699.598234	16.590285
28.639219	1706.552393	16.595303
28.950191	1712.080461	16.600320
29.095422	1703.319842	16.605338
28.554900	1684.036585	16.610355
28.689709	1691.066255	16.615373
28.887748	1697.242152	16.620391
28.701018	1699.179803	16.625408
28.619883	1700.119261	16.630426
28.909310	1697.826099	16.635443
28.979603	1704.153467	16.640461
29.047581	1704.428470	16.645479
29.070369	1706.263316	16.650496
28.810623	1706.359124	16.655514
28.958941	1702.160591	16.660531
28.609935	1704.951492	16.665549
29.010221	1695.594311	16.670567
28.866981	1697.912949	16.675584
28.914085	1694.448893	16.680602
29.095667	1696.883427	16.685619
28.644153	1699.821223	16.690637
29.140516	1696.237890	16.695655
29.211068	1700.898287	16.700672
28.766530	1692.628645	16.705690
29.350882	1695.286637	16.710707
29.557500	1712.680792	16.715725
29.504225	1701.356590	16.720743
29.495973	1704.659174	16.725760
29.322934	1702.103224	16.730778
29.462350	1692.593969	16.735795
29.490627	1701.087345	16.740813
29.372034	1694.099552	16.745831
29.511133	1697.816315	16.750848
29.399484	1698.787598	16.755866
29.932766	1705.544202	16.760883
29.653774	1711.858154	16.765901
29.491772	1686.843712	16.770919
29.581379	1698.954877	16.775936
29.433744	1710.480535	16.780954
30.027371	1711.833846	16.785971
29.748118	1707.390367	16.790989
29.941849	1720.094936	16.796007
29.731289	1713.531418	16.801024
29.778351	1718.096498	16.806042
30.222314	1712.026169	16.811059
29.999968	1713.442555	16.816077
29.886315	1696.420878	16.821095
29.842721	1694.007667	16.826112
29.855146	1702.304063	16.831130
30.103373	1703.811027	16.836147
30.107500	1714.164707	16.841165
30.159263	1707.148304	16.846183
30.021643	1712.101445	16.851200
30.253103	1710.336384	16.856218
30.295417	1713.493982	16.861235
29.824945	1712.651457	16.866253
30.251938	1702.341818	16.871271
30.371072	1707.315039	16.876288
30.100146	1707.459942	16.881306
30.331205	1709.489040	16.886323
30.427770	1714.883716	16.891341
30.352920	1702.793402	16.896359
30.551535	1702.683779	16.901376
30.330408	1701.294847	16.906394
29.717738	1695.734538	16.911411
29.974351	1709.388132	16.916429
30.099197	1706.980491	16.921447
30.336837	1701.907718	16.926464
29.912768	1705.632702	16.931482
30.409664	1727.375258	16.936499
30.568521	1741.622235	16.941517
30.754997	1732.822092	16.946535
30.489041	1733.400031	16.951552
30.577350	1738.877973	16.956570
31.362762	1725.902664	16.961587
30.761521	1727.235337	16.966605
30.981158	1725.543886	16.971623
30.965788	1727.204739	16.976640
30.924849	1740.203303	16.981658
31.051933	1729.626380	16.986675
31.139793	1724.950844	16.991693
30.957341	1725.821254	16.996711
30.856543	1723.094677	17.001728
30.895557	1730.614638	17.006746
31.021124	1721.381280	17.011763
30.828537	1729.959672	17.016781
31.135996	1733.489115	17.021799
31.308772	1724.416836	17.026816
31.053739	1731.385490	17.031834
31.402005	1723.110136	17.036851
30.874729	1730.265210	17.041869
31.183861	1730.303823	17.046887
31.253964	1734.052493	17.051904
31.307657	1736.537344	17.056922
31.166528	1726.094603	17.061939
30.919960	1728.523269	17.066957
30.991389	1721.658327	17.071975
31.282617	1738.309759	17.076992
31.034288	1757.106862	17.082010
31.593012	1753.043503	17.087027
31.789277	1763.504770	17.092045
31.537195	1756.761101	17.097063
31.748157	1761.205352	17.102080
31.517966	1769.405739	17.107098
31.498673	1753.112471	17.112115
31.667242	1758.063348	17.117133
31.429405	1757.456707	17.122151
31.850355	1765.231942	17.127168
31.453131	1762.690272	17.132186
31.577782	1760.260214	17.137203
31.698501	1758.372147	17.142221
31.535008	1758.873277	17.147239
31.715375	1758.374549	17.152256
32.163178	1781.542638	17.157274
32.169441	1782.607393	17.162291
31.821375	1778.866236	17.167309
32.039473	1784.924672	17.172327
32.467804	1778.332889	17.177344
32.151768	1759.834413	17.182362
32.112598	1750.717295	17.187379
32.086626	1755.696055	17.192397
32.329372	1762.645286	17.197415
32.451212	1757.147968	17.202432
31.826595	1754.382930	17.207450
32.389743	1761.464536	17.212467
32.364729	1777.736488	17.217485
32.261459	1780.347339	17.222503
32.706705	1770.432273	17.227520
32.484938	1768.415879	17.232538
32.399858	1751.431930	17.237555
32.195192	1765.884402	17.242573
32.246848	1774.642846	17.247591
32.433998	1774.381972	17.252608
32.376130	1781.168391	17.257626
32.772172	1777.936300	17.262643
32.711695	1783.257399	17.267661
32.717255	1777.741141	17.272679
32.843602	1776.885608	17.277696
32.883909	1771.931711	17.282714
32.672436	1780.765227	17.287731
32.251325	1783.186978	17.292749
32.689413	1779.018392	17.297767
32.610609	1771.643265	17.302784
32.917919	1779.863312	17.307802
32.906082	1773.620799	17.312819
32.622818	1773.335067	17.317837
32.517073	1774.597897	17.322855
32.544364	1778.851701	17.327872
32.793294	1797.462571	17.332890
33.156360	1788.433941	17.337907
33.180503	1805.742669	17.342925
33.431958	1802.046717	17.347943
33.403686	1790.437206	17.352960
33.031949	1804.076038	17.357978
33.285659	1802.700592	17.362995
33.077585	1804.470923	17.368013
33.189775	1796.708643	17.373031
33.772424	1791.773985	17.378048
33.241052	1798.751815	17.383066
33.376971	1789.767098	17.388083
33.474038	1801.731438	17.393101
33.369990	1796.916398	17.398119
33.793952	1788.028472	17.403136
33.289087	1790.848741	17.408154
33.682361	1796.593133	17.413171
33.536807	1796.676725	17.418189
33.293368	1796.269436	17.423207
33.653175	1786.446461	17.428224
33.284184	1792.419835	17.433242
33.723829	1810.112521	17.438259
33.845134	1820.720492	17.443277
33.559341	1827.131680	17.448295
33.990801	1818.035801	17.453312
33.839793	1820.008890	17.458330
33.838198	1822.783622	17.463347
34.514877	1818.449137	17.468365
34.089661	1821.347561	17.473383
34.251953	1814.145877	17.478400
33.853161	1802.499287	17.483418
34.194752	1808.169564	17.488435
34.482848	1806.633699	17.493453
34.194860	1799.482175	17.498471
34.210717	1779.955876	17.503488
34.002722	1793.712859	17.508506
34.414199	1793.547122	17.513523
34.314234	1797.839720	17.518541
34.065432	1813.841680	17.523559
34.458178	1810.510915	17.528576
34.334140	1818.140596	17.533594
34.558694	1814.741224	17.538611
34.804027	1809.173833	17.543629
34.469560	1815.089923	17.548647
34.761565	1800.621445	17.553664
34.661828	1793.415522	17.558682
34.542284	1780.535300	17.563699
34.365422	1779.302417	17.568717
34.396092	1801.060077	17.573735
34.762683	1802.309260	17.578752
34.570123	1819.125539	17.583770
34.919701	1801.863256	17.588787
34.778287	1807.779659	17.593805
34.962834	1814.016892	17.598823
35.141895	1805.943531	17.603840
34.663589	1811.213750	17.608858
34.486744	1806.130839	17.613875
34.447342	1808.835450	17.618893
34.443233	1806.815686	17.623911
34.623362	1802.858315	17.628928
34.655910	1814.441222	17.633946
35.113235	1829.248701	17.638963
34.928817	1846.154999	17.643981
35.148144	1836.975339	17.648999
35.339621	1836.216893	17.654016
35.192804	1841.398765	17.659034
35.158005	1842.863240	17.664051
35.499700	1842.007871	17.669069
34.727488	1846.183455	17.674087
35.177884	1838.670662	17.679104
35.123034	1844.387310	17.684122
35.138331	1841.323768	17.689139
35.060465	1836.666586	17.694157
35.103512	1862.613260	17.699175
35.724877	1863.073008	17.704192
35.631406	1871.227974	17.709210
35.838548	1866.809810	17.714227
36.213213	1860.929642	17.719245
36.231005	1847.393151	17.724263
36.208220	1830.335807	17.729280
35.969428	1828.936402	17.734298
35.806024	1822.604794	17.739315
36.168149	1822.660616	17.744333
35.801200	1832.860862	17.749351
36.210218	1817.309205	17.754368
35.993940	1826.087243	17.759386
36.208380	1819.534798	17.764403
35.974303	1818.000754	17.769421
35.996316	1822.285759	17.774439
36.207231	1816.932333	17.779456
35.627640	1818.254341	17.784474
35.796570	1823.302031	17.789491
36.185383	1817.651034	17.794509
36.186213	1816.115099	17.799527
36.062176	1817.049069	17.804544
35.994202	1828.949421	17.809562
36.079106	1836.404354	17.814579
36.161930	1844.460427	17.819597
36.033475	1850.814467	17.824615
36.641677	1854.654771	17.829632
36.509694	1850.103397	17.834650
36.343357	1850.128225	17.839667
36.701086	1852.703301	17.844685
36.493853	1858.929050	17.849703
36.488831	1861.159469	17.854720
36.393436	1857.253222	17.859738
36.628468	1852.000909	17.864755
36.591893	1848.509338	17.869773
36.342214	1853.408244	17.874791
36.874805	1862.520566	17.879808
36.635314	1876.517486	17.884826
36.734374	1878.773586	17.889843
37.073311	1874.454070	17.894861
36.864090	1881.142367	17.899879
37.022886	1875.098725	17.904896
37.075705	1878.273515	17.909914
37.053625	1876.079550	17.914931
37.148947	1862.970763	17.919949
37.319277	1876.094693	17.924967
37.453026	1872.313491	17.929984
37.061926	1876.085418	17.935002
37.400393	1870.885657	17.940019
37.645403	1867.407689	17.945037
37.647430	1847.167840	17.950055
37.392021	1843.221952	17.955072
37.384352	1839.267717	17.960090
37.506394	1834.743181	17.965107
37.610208	1839.994181	17.970125
37.185512	1837.633032	17.975143
37.299975	1825.155364	17.980160
37.267332	1838.010509	17.985178
37.611036	1852.598635	17.990195
37.688310	1867.153334	17.995213
37.283559	1863.886114	18.000231
37.455193	1858.784456	18.005248
38.060998	1857.661728	18.010266
37.705576	1853.256803	18.015283
37.828727	1861.711329	18.020301
37.338499	1863.048070	18.025319
37.488608	1864.431139	18.030336
37.523783	1862.476517	18.035354
37.715589	1866.003095	18.040371
38.289640	1883.361007	18.045389
37.868905	1895.706050	18.050407
38.187766	1884.845688	18.055424
38.199270	1894.220697	18.060442
37.997604	1886.273334	18.065459
38.402186	1885.098097	18.070477
38.144708	1898.622420	18.075495
38.311048	1888.797953	18.080512
38.388244	1892.956121	18.085530
38.268948	1893.079066	18.090547
38.288963	1886.052091	18.095565
38.085350	1888.702411	18.100583
38.274676	1881.968664	18.105600
38.371773	1886.244009	18.110618
38.143539	1887.324374	18.115635
38.410436	1883.186471	18.120653
38.248808	1897.420126	18.125671
38.525559	1904.161424	18.130688
38.687407	1912.296968	18.135706
38.372629	1922.464223	18.140723
38.808685	1904.190643	18.145741
38.408105	1915.949680	18.150759
38.456715	1916.261359	18.155776
38.693486	1915.070994	18.160794
38.594509	1907.029055	18.165811
39.162556	1917.874537	18.170829
39.128591	1935.600518	18.175847
39.333261	1923.463350	18.180864
39.328267	1912.906993	18.185882
38.815646	1909.609593	18.190899
39.525079	1895.189623	18.195917
39.282377	1917.550989	18.200935
39.181857	1905.793117	18.205952
39.567222	1910.477038	18.210970
39.444256	1911.379734	18.215987
39.414105	1911.854457	18.221005
39.390506	1913.236374	18.226023
39.583526	1905.687035	18.231040
39.614093	1902.747725	18.236058
39.006086	1908.233550	18.241075
39.372718	1900.514124	18.246093
39.272546	1907.665876	18.251111
39.443777	1924.208638	18.256128
39.743897	1933.463437	18.261146
39.427201	1936.656120	18.266163
39.604181	1940.983214	18.271181
39.780031	1937.463138	18.276199
39.595297	1941.457998	18.281216
39.584529	1933.594355	18.286234
39.738340	1940.524927	18.291251
39.989062	1929.989601	18.296269
39.744596	1927.938361	18.301287
40.127920	1931.255679	18.306304
40.024331	1927.014152	18.311322
40.104455	1934.066375	18.316339
40.024186	1932.730081	18.321357
39.801273	1932.435138	18.326375
40.101296	1926.224782	18.331392
40.306607	1931.919247	18.336410
40.466235	1952.021884	18.341427
40.506746	1951.541979	18.346445
40.618463	1940.679265	18.351463
40.415972	1935.889144	18.356480
40.553543	1930.782868	18.361498
40.335816	1930.914238	18.366515
40.127650	1939.502411	18.371533
40.209010	1950.099762	18.376551
40.530533	1961.023499	18.381568
40.864733	1952.420821	18.386586
40.289916	1970.066322	18.391603
40.448751	1959.188705	18.396621
40.558432	1964.793899	18.401639
40.234043	1965.937435	18.406656
40.861012	1967.495884	18.411674
40.988585	1981.042739	18.416691
40.971579	1977.852627	18.421709
40.702647	1979.092495	18.426727
41.182786	1984.849739	18.431744
41.313399	1979.453255	18.436762
41.153912	1990.439342	18.441779
41.482385	1976.177658	18.446797
41.168727	1955.644269	18.451815
40.943127	1966.110175	18.456832
41.346405	1966.602105	18.461850
41.250003	1972.500486	18.466867
41.478649	1969.287808	18.471885
41.665023	1976.273636	18.476903
41.557410	1972.710333	18.481920
41.701925	1966.006018	18.486938
41.737887	1957.442094	18.491955
41.566671	1941.271424	18.496973
41.258451	1946.911167	18.501991
41.662831	1957.205424	18.507008
41.852795	1961.301629	18.512026
41.919019	1976.670085	18.517043
41.484059	1955.109521	18.522061
41.845962	1965.397825	18.527079
41.618811	1972.159603	18.532096
42.190955	1973.945245	18.537114
41.939210	1976.226379	18.542131
41.573979	1978.068423	18.547149
41.904395	1974.566053	18.552167
41.404129	1976.435576	18.557184
41.729567	1972.508432	18.562202
41.552240	1974.200068	18.567219
41.677956	1979.089607	18.572237
41.795686	1996.717702	18.577255
41.847299	1998.854115	18.582272
42.398725	1996.981708	18.587290
42.117602	2011.271081	18.592307
42.665168	2003.139352	18.597325
42.457763	2000.054782	18.602343
42.534090	2006.807267	18.607360
42.355508	2001.795840	18.612378
42.397780	1999.604193	18.617395
42.331548	2004.719231	18.622413
42.356203	1999.904075	18.627431
41.990130	2003.658502	18.632448
42.540980	2006.800848	18.637466
42.345110	2022.246609	18.642483
42.761748	2025.124958	18.647501
42.696501	2023.649158	18.652519
43.116540	2026.793485	18.657536
43.489855	2028.080945	18.662554
42.898873	2029.099731	18.667571
43.305277	2018.808255	18.672589
43.622708	2017.459248	18.677607
42.910835	2019.058693	18.682624
43.588221	1999.050126	18.687642
43.696336	1996.197171	18.692659
42.985169	1985.891956	18.697677
43.370112	1984.219169	18.702695
43.074725	1981.244054	18.707712
43.386161	1975.595577	18.712730
43.166111	1992.624079	18.717747
43.459433	1998.169741	18.722765
43.900290	2006.418584	18.727783
43.356926	2010.169298	18.732800
43.582532	1997.227804	18.737818
44.161377	2004.165584	18.742835
43.433553	1992.966649	18.747853
43.608143	1990.086152	18.752871
43.423936	2010.165484	18.757888
44.031782	2005.663211	18.762906
43.716743	2015.574660	18.767923
43.693068	2025.992602	18.772941
43.977116	2019.461226	18.777959
43.643609	2022.302766	18.782976
43.935453	2016.067350	18.787994
44.277628	2018.972989	18.793011
43.834624	2017.239265	18.798029
44.147019	2008.546071	18.803047
43.895077	2018.449829	18.808064
43.920427	2015.131039	18.813082
43.837746	2017.126698	18.818099
44.180571	2022.551964	18.823117
44.418375	2030.324197	18.828135
44.159448	2039.658247	18.833152
44.647524	2034.361610	18.838170
44.690894	2032.737111	18.843187
44.118647	2031.811417	18.848205
44.408201	2040.836529	18.853223
44.221659	2030.037315	18.858240
44.396423	2031.994281	18.863258
44.316648	2030.859870	18.868275
43.905825	2036.450491	18.873293
44.380876	2043.876746	18.878311
44.471143	2059.144449	18.883328
44.828199	2057.987307	18.888346
44.918981	2069.925336	18.893363
44.724406	2069.383960	18.898381
44.959390	2062.311465	18.903399
45.108028	2065.616493	18.908416
45.087772	2066.073440	18.913434
44.851708	2057.653327	18.918451
44.757862	2063.500531	18.923469
45.217232	2069.835276	18.928487
45.167103	2090.700796	18.933504
45.513678	2080.889277	18.938522
45.531533	2081.598187	18.943539
45.077295	2081.903765	18.948557
45.428295	2080.362969	18.953575
45.383779	2086.988646	18.958592
45.575466	2082.743064	18.963610
45.367598	2083.541322	18.968627
45.450782	2081.181468	18.973645
45.425996	2078.307198	18.978663
45.666945	2075.262150	18.983680
45.680628	2071.457868	18.988698
45.864251	2079.751708	18.993715
45.660678	2079.140167	18.998733
45.796583	2075.606990	19.003751
45.735606	2080.405820	19.008768
45.869915	2073.557083	19.013786
45.968381	2078.633848	19.018803
45.765465	2096.464369	19.023821
46.230304	2095.154333	19.028839
46.473945	2104.602844	19.033856
46.415825	2101.884880	19.038874
46.599559	2088.342355	19.043891
46.542781	2071.801803	19.048909
46.703429	2060.416324	19.053927
46.565701	2060.096249	19.058944
46.703608	2055.762333	19.063962
46.740005	2060.562356	19.068979
46.660594	2062.061405	19.073997
46.713964	2053.572893	19.079015
46.377804	2054.370739	19.084032
46.704946	2057.755264	19.089050
46.759272	2054.827740	19.094067
46.581362	2064.085002	19.099085
46.548338	2054.253285	19.104103
46.393481	2067.140669	19.109120
46.618783	2078.883591	19.114138
46.662503	2085.652140	19.119155
46.961155	2092.372178	19.124173
46.827023	2090.106971	19.129191
46.980750	2098.767986	19.134208
47.000782	2089.806617	19.139226
46.861264	2092.197926	19.144243
46.631620	2096.351840	19.149261
47.082266	2099.660803	19.154279
47.322004	2118.531463	19.159296
47.193434	2121.859571	19.164314
47.400196	2122.819886	19.169331
47.340279	2133.659267	19.174349
47.295771	2123.063246	19.179367
47.440901	2120.852188	19.184384
47.104487	2121.714255	19.189402
47.451018	2118.028471	19.194419
47.586386	2133.156886	19.199437
47.892075	2141.964419	19.204455
47.709533	2148.677547	19.209472
47.784475	2147.017493	19.214490
48.341489	2153.596741	19.219507
48.212994	2143.108711	19.224525
48.300308	2122.065777	19.229543
48.028758	2110.046693	19.234560
47.931143	2104.711975	19.239578
48.192982	2112.403890	19.244595
47.863307	2129.182183	19.249613
48.231481	2132.858757	19.254631
48.057496	2128.201655	19.259648
48.033489	2138.802803	19.264666
48.048573	2131.602120	19.269683
48.257153	2148.608634	19.274701
48.530039	2137.651770	19.279719
48.447978	2137.111445	19.284736
48.205620	2142.043876	19.289754
48.051824	2133.882940	19.294771
48.528097	2145.848141	19.299789
48.729634	2160.144736	19.304807
48.594556	2166.960252	19.309824
48.685445	2163.124658	19.314842
49.182545	2165.526705	19.319859
49.026598	2166.676616	19.324877
49.192650	2163.358118	19.329895
48.938841	2169.707061	19.334912
48.984172	2158.422104	19.339930
49.021967	2164.290856	19.344947
49.023128	2159.703170	19.349965
48.962321	2155.957266	19.354983
49.233066	2165.452115	19.360000
49.155823	2160.159674	19.365018
49.480289	2155.179861	19.370035
48.998829	2159.749910	19.375053
49.250289	2153.534119	19.380071
49.328641	2156.267718	19.385088
49.354741	2162.330537	19.390106
49.272629	2161.865813	19.395123
49.581930	2172.216117	19.400141
49.754564	2181.232325	19.405159
49.858508	2193.945064	19.410176
49.640878	2195.823324	19.415194
49.975283	2194.586456	19.420211
49.728855	2190.068501	19.425229
49.819608	2186.440410	19.430247
49.984339	2197.552882	19.435264
50.066498	2186.553154	19.440282
50.029883	2191.401922	19.445299
50.060427	2184.676228	19.450317
50.084264	2184.926264	19.455335
50.145048	2186.554870	19.460352
50.153595	2183.841995	19.465370
50.440667	2185.172492	19.470387
50.270883	2192.947337	19.475405
50.332742	2189.761446	19.480423
50.367469	2193.905074	19.485440
50.438838	2197.660734	19.490458
50.586576	2180.667290	19.495475
50.460766	2183.953614	19.500493
50.751100	2193.725559	19.505511
50.560596	2194.017388	19.510528
50.411360	2208.579994	19.515546
50.906666	2205.738873	19.520563
50.679200	2207.860108	19.525581
50.838860	2208.811693	19.530599
50.961457	2215.252266	19.535616
50.980947	2208.705169	19.540634
50.885814	2200.563619	19.545651
50.986162	2215.221914	19.550669
50.975452	2202.808767	19.555687
50.897322	2202.365430	19.560704
50.956213	2215.147067	19.565722
51.146604	2222.117380	19.570739
51.238618	2237.293234	19.575757
51.537720	2229.641524	19.580775
51.904448	2227.553998	19.585792
51.700342	2239.211449	19.590810
51.643239	2235.587358	19.595827
51.311416	2234.898224	19.600845
51.600153	2234.665800	19.605863
51.589511	2225.335797	19.610880
51.347467	2229.148875	19.615898
51.719693	2230.839697	19.620915
51.769439	2236.765948	19.625933
51.841454	2227.114766	19.630951
52.216661	2232.895781	19.635968
52.026367	2240.194503	19.640986
52.130153	2229.569522	19.646003
52.196523	2233.570121	19.651021
52.133837	2229.164253	19.656039
52.184004	2229.034721	19.661056
52.071184	2230.801531	19.666074
52.143100	2221.619282	19.671091
52.331184	2240.372262	19.676109
52.396987	2247.782916	19.681127
52.695623	2253.266765	19.686144
52.459105	2264.000436	19.691162
52.758982	2257.408464	19.696179
52.482723	2269.721215	19.701197
52.458333	2255.091315	19.706215
52.748103	2263.494060	19.711232
52.712206	2258.967994	19.716250
52.818094	2248.026107	19.721267
52.766562	2252.531684	19.726285
52.612384	2250.998145	19.731303
52.495154	2251.160120	19.736320
52.860080	2254.036447	19.741338
52.856714	2268.099740	19.746355
52.968314	2279.094685	19.751373
53.461814	2282.189893	19.756391
53.473506	2279.171744	19.761408
53.158972	2279.686482	19.766426
53.478239	2277.496963	19.771443
53.359773	2277.618591	19.776461
53.384823	2278.899174	19.781479
53.852342	2278.022161	19.786496
53.414196	2275.900186	19.791514
53.714958	2274.024372	19.796531
53.450463	2272.972500	19.801549
53.482294	2273.857852	19.806567
53.805066	2267.313267	19.811584
53.866184	2283.734091	19.816602
53.864642	2282.604423	19.821619
53.886269	2299.906638	19.826637
54.106376	2297.229973	19.831655
54.196373	2298.256487	19.836672
54.176885	2297.548703	19.841690
54.735439	2288.760653	19.846707
54.638604	2287.019576	19.851725
54.229400	2275.140879	19.856743
54.270346	2266.995659	19.861760
54.452715	2283.257423	19.866778
54.542634	2284.721760	19.871795
54.464962	2290.910084	19.876813
54.552978	2289.202573	19.881831
54.578115	2289.715004	19.886848
54.662719	2292.858631	19.891866
54.690587	2276.804650	19.896883
54.276529	2286.939761	19.901901
54.413076	2284.674981	19.906919
54.976901	2279.693290	19.911936
54.502478	2277.401724	19.916954
55.008333	2282.178017	19.921971
54.643244	2289.497832	19.926989
54.804256	2311.989377	19.932007
55.248624	2307.316446	19.937024
54.945785	2317.194567	19.942042
55.353020	2316.841335	19.947059
55.242444	2311.700037	19.952077
55.235201	2311.559144	19.957095
55.253594	2318.783975	19.962112
55.052797	2323.190268	19.967130
55.205070	2311.759140	19.972147
55.349012	2320.281342	19.977165
55.293938	2334.932808	19.982183
55.758007	2341.839746	19.987200
55.483968	2347.594843	19.992218
55.714932	2352.689916	19.997235
55.767084	2339.039036	20.002253
55.989646	2342.843713	20.007271
55.813003	2342.837568	20.012288
55.638891	2346.008691	20.017306
56.310593	2346.797540	20.022323
56.052752	2342.030238	20.027341
56.070110	2340.626559	20.032359
56.637902	2340.795581	20.037376
56.239284	2343.463306	20.042394
56.406767	2341.810350	20.047411
55.936801	2351.243313	20.052429
56.295595	2361.829653	20.057447
56.777804	2361.969538	20.062464
56.682856	2373.938949	20.067482
56.806004	2373.815049	20.072499
56.844756	2364.214962	20.077517
56.621354	2369.088810	20.082535
57.066838	2366.557499	20.087552
56.799579	2363.310317	20.092570
56.845186	2366.268282	20.097587
57.052251	2367.106117	20.102605
56.870512	2363.984150	20.107623
57.136549	2357.370179	20.112640
56.968783	2363.352182	20.117658
57.138713	2366.597447	20.122675
57.183981	2363.695775	20.127693
57.097967	2370.732005	20.132711
57.466243	2369.185566	20.137728
57.422656	2368.343968	20.142746
57.155564	2376.635433	20.147763
57.403388	2379.132732	20.152781
57.186296	2386.236738	20.157799
57.238428	2386.638399	20.162816
57.568295	2389.750487	20.167834
57.400234	2385.661643	20.172851
57.794995	2392.108406	20.177869
57.726500	2404.147873	20.182887
58.025800	2408.642253	20.187904
57.728637	2403.537728	20.192922
58.213208	2407.753780	20.197939
58.468175	2404.850449	20.202957
58.206791	2404.490210	20.207975
58.202674	2405.030324	20.212992
58.085327	2405.683287	20.218010
58.269791	2400.295065	20.223027
58.163625	2404.082535	20.228045
58.512658	2408.114723	20.233063
58.616477	2399.036541	20.238080
58.464312	2399.542900	20.243098
58.505996	2400.797903	20.248115
58.664662	2406.772722	20.253133
58.583437	2424.397632	20.258151
58.801210	2423.672996	20.263168
58.734386	2431.268699	20.268186
58.844903	2424.154050	20.273203
59.394500	2420.355828	20.278221
59.087523	2420.875617	20.283239
59.326454	2415.501206	20.288256
59.149233	2419.552819	20.293274
59.296897	2424.670372	20.298291
59.285986	2416.384836	20.303309
59.201917	2416.966538	20.308327
59.470810	2418.458734	20.313344
59.508720	2415.233453	20.318362
59.518019	2416.161128	20.323379
59.525393	2420.643220	20.328397
59.666695	2420.105271	20.333415
59.556851	2407.156382	20.338432
59.475473	2415.452550	20.343450
59.816714	2410.898244	20.348467
59.576090	2409.354593	20.353485
59.436153	2417.145081	20.358503
59.802729	2435.710466	20.363520
59.708257	2450.778820	20.368538
59.830155	2448.091225	20.373555
60.017825	2452.824980	20.378573
59.811594	2448.247534	20.383591
59.747608	2451.224844	20.388608
59.589664	2471.321288	20.393626
60.213267	2470.440469	20.398643
60.454261	2478.514383	20.403661
60.225866	2476.605690	20.408679
60.511096	2475.973430	20.413696
60.659626	2479.780558	20.418714
60.655356	2464.618757	20.423731
60.636527	2486.813154	20.428749
61.105962	2493.580289	20.433767
61.151412	2494.229134	20.438784
61.003465	2498.220799	20.443802
60.884469	2492.444583	20.448819
61.292202	2485.624015	20.453837
61.050853	2490.593003	20.458855
61.458385	2488.856186	20.463872
61.259881	2482.447438	20.468890
61.745062	2476.831826	20.473907
61.508927	2480.912109	20.478925
61.284349	2485.964937	20.483943
61.985105	2478.141867	20.488960
61.721235	2479.947497	20.493978
61.427413	2481.880928	20.498995
61.398106	2473.422808	20.504013
61.105037	2486.646038	20.509031
61.629843	2479.949007	20.514048
61.975535	2475.986101	20.519066
61.765724	2486.071770	20.524083
61.976784	2483.096163	20.529101
61.736708	2487.727915	20.534119
61.991242	2498.235546	20.539136
61.804142	2518.843598	20.544154
61.880696	2520.486558	20.549171
62.446683	2517.366736	20.554189
62.179737	2517.775957	20.559207
62.301873	2507.080817	20.564224
62.262245	2512.348710	20.569242
62.115164	2525.542287	20.574259
62.507733	2529.910229	20.579277
62.348020	2540.571526	20.584295
62.715875	2536.813214	20.589312
62.725293	2545.846424	20.594330
62.798046	2542.414155	20.599347
62.961218	2543.797880	20.604365
62.618023	2549.151094	20.609383
62.699319	2548.070685	20.614400
63.424385	2559.513882	20.619418
63.140436	2566.560139	20.624435
63.278476	2561.726823	20.629453
63.593685	2570.176706	20.634471
63.630384	2556.677020	20.639488
63.628386	2551.138903	20.644506
63.441039	2543.756971	20.649523
63.547943	2542.119536	20.654541
63.542014	2536.482464	20.659559
63.749169	2562.372029	20.664576
63.800088	2565.252770	20.669594
63.794921	2562.603127	20.674611
64.012158	2562.063230	20.679629
63.709369	2567.379442	20.684647
63.662921	2563.221197	20.689664
63.765423	2565.068144	20.694682
63.762184	2566.190828	20.699699
63.759453	2555.070638	20.704717
63.738497	2560.410656	20.709735
64.236579	2576.688170	20.714752
64.123628	2589.795830	20.719770
64.034849	2584.762649	20.724787
64.540252	2585.488100	20.729805
64.448894	2597.109038	20.734823
64.678028	2584.919271	20.739840
64.588719	2581.963854	20.744858
64.957643	2583.603686	20.749875
64.817251	2576.460433	20.754893
64.931038	2597.541236	20.759911
64.898642	2579.102299	20.764928
64.858386	2586.596035	20.769946
65.007705	2594.950560	20.774963
65.171727	2601.104498	20.779981
65.394897	2603.052341	20.784999
65.529803	2609.980833	20.790016
65.533651	2600.365513	20.795034
65.689504	2601.369724	20.800051
65.700208	2591.246159	20.805069
65.398239	2590.216612	20.810087
65.895329	2590.476878	20.815104
65.631256	2592.580209	20.820122
65.601269	2602.998402	20.825139
65.883385	2596.262764	20.830157
65.728856	2600.340983	20.835175
65.871544	2591.334997	20.840192
65.920278	2583.185960	20.845210
65.830989	2597.408275	20.850227
66.259048	2590.402396	20.855245
65.634390	2591.649635	20.860263
66.018468	2590.729335	20.865280
66.750866	2604.469514	20.870298
66.130546	2611.251786	20.875315
66.465505	2613.048829	20.880333
66.136755	2622.956632	20.885351
66.528847	2621.367247	20.890368
66.799016	2624.769601	20.895386
66.562334	2625.204130	20.900403
67.020260	2626.807968	20.905421
66.402465	2617.015242	20.910439
66.880146	2618.005537	20.915456
66.714505	2622.665950	20.920474
66.692477	2630.902796	20.925491
66.947002	2642.073556	20.930509
67.093670	2651.260490	20.935527
66.970282	2651.176623	20.940544
67.488749	2652.199933	20.945562
67.623586	2650.312178	20.950579
67.626462	2637.070401	20.955597
67.471375	2646.452582	20.960615
67.556873	2638.373417	20.965632
67.728534	2636.144901	20.970650
67.335538	2640.451605	20.975667
68.047754	2638.568646	20.980685
67.777063	2635.396782	20.985703
67.756401	2631.685063	20.990720
67.781410	2640.680311	20.995738
67.444059	2649.909987	21.000755
67.713037	2658.305759	21.005773
68.239326	2671.064317	21.010791
67.991140	2678.728362	21.015808
67.973722	2668.190086	21.020826
68.275497	2679.796778	21.025843
68.561715	2670.677605	21.030861
68.079436	2671.944190	21.035879
68.291048	2691.728134	21.040896
68.565141	2694.286888	21.045914
68.750597	2709.402452	21.050931
68.997817	2692.127394	21.055949
68.961557	2692.288959	21.060967
68.760536	2704.021054	21.065984
69.050239	2709.063603	21.071002
68.609790	2701.446716	21.076019
68.993039	2698.286642	21.081037
69.043057	2699.347758	21.086055
68.947979	2708.316077	21.091072
68.856297	2720.106068	21.096090
69.179507	2728.559044	21.101107
69.508714	2721.233627	21.106125
69.659201	2733.244175	21.111143
69.518623	2729.245183	21.116160
69.768907	2726.769762	21.121178
69.586811	2727.355108	21.126195
69.566540	2718.907169	21.131213
69.830733	2726.590733	21.136231
70.037565	2735.134248	21.141248
70.305348	2734.192643	21.146266
69.990533	2743.052476	21.151283
70.259914	2733.952197	21.156301
70.642181	2739.297166	21.161319
70.406369	2735.537578	21.166336
70.518477	2733.990607	21.171354
70.606626	2739.424832	21.176371
70.622617	2734.994374	21.181389
70.430729	2733.204415	21.186407
70.626717	2741.608775	21.191424
70.888473	2727.489747	21.196442
70.972629	2739.611683	21.201459
70.663746	2729.601975	21.206477
70.805239	2730.382180	21.211495
70.884138	2728.159168	21.216512
70.575538	2723.457243	21.221530
71.054265	2751.883425	21.226547
71.359654	2760.255112	21.231565
71.091361	2763.639171	21.236583
71.005920	2762.785190	21.241600
71.465995	2761.469200	21.246618
71.287099	2761.027570	21.251635
71.419342	2759.569395	21.256653
71.305907	2757.149471	21.261671
71.505673	2773.534861	21.266688
71.716259	2782.450247	21.271706
71.759049	2780.758833	21.276723
72.063111	2776.801171	21.281741
71.889904	2789.409886	21.286759
71.837485	2785.372658	21.291776
71.821978	2777.992082	21.296794
71.441383	2793.134131	21.301811
72.034194	2801.050738	21.306829
72.031691	2807.113426	21.311847
71.980660	2814.993335	21.316864
72.501697	2808.003856	21.321882
72.430937	2805.300855	21.326899
72.656556	2807.376675	21.331917
73.108511	2800.523057	21.336935
73.110119	2800.357070	21.341952
73.030603	2801.679029	21.346970
72.835622	2809.989492	21.351987
73.322766	2802.725293	21.357005
73.403850	2798.786436	21.362023
73.259884	2802.148341	21.367040
73.324790	2805.831198	21.372058
72.953862	2802.815671	21.377075
72.919817	2802.170908	21.382093
73.359790	2810.922334	21.387111
73.408916	2831.184969	21.392128
73.770715	2823.570623	21.397146
73.649550	2830.629022	21.402163
73.674691	2830.183135	21.407181
73.692459	2822.424167	21.412199
73.657550	2828.505222	21.417216
73.965371	2825.868673	21.422234
73.638221	2828.548268	21.427251
73.696205	2831.245592	21.432269
74.076101	2843.383211	21.437287
73.931870	2850.650572	21.442304
74.112916	2841.542021	21.447322
74.153123	2853.007889	21.452339
74.182703	2849.024000	21.457357
74.703958	2855.099594	21.462375
74.367220	2877.404279	21.467392
74.779315	2878.044796	21.472410
74.544742	2882.279659	21.477427
74.751873	2882.412736	21.482445
74.916102	2884.126657	21.487463
74.976016	2881.031898	21.492480
75.007269	2880.568854	21.497498
75.000078	2884.490850	21.502515
74.968808	2879.003924	21.507533
75.084772	2897.115653	21.512551
75.269947	2906.930661	21.517568
75.601226	2908.913796	21.522586
75.513213	2918.009422	21.527603
75.686595	2913.822557	21.532621
75.733321	2901.708815	21.537639
75.307631	2907.716803	21.542656
75.622747	2910.286124	21.547674
75.842105	2904.643901	21.552691
75.560389	2914.331484	21.557709
76.007345	2915.382403	21.562727
75.979997	2930.405851	21.567744
76.129425	2924.267680	21.572762
76.012132	2926.731819	21.577779
75.952759	2930.677822	21.582797
76.211371	2932.171773	21.587815
76.153828	2947.686496	21.592832
76.746815	2948.030900	21.597850
76.635743	2959.236046	21.602867
76.604984	2956.797677	21.607885
76.763761	2953.707008	21.612903
76.521903	2968.019495	21.617920
76.951292	2959.039453	21.622938
77.062276	2954.420355	21.627955
76.875015	2949.753391	21.632973
77.241788	2958.836732	21.637991
77.064748	2972.464815	21.643008
77.419544	2962.087953	21.648026
77.598909	2969.237215	21.653043
77.639340	2975.266085	21.658061
77.826517	2973.129449	21.663079
78.071347	2983.080309	21.668096
78.006073	2965.687388	21.673114
78.185752	2958.976038	21.678131
77.876511	2946.938527	21.683149
77.974222	2934.702922	21.688167
78.004249	2936.417022	21.693184
78.049349	2948.120357	21.698202
78.227492	2958.078306	21.703219
78.265357	2971.820816	21.708237
78.402229	2975.467778	21.713255
78.150685	2967.163127	21.718272
78.329323	2971.909956	21.723290
78.392737	2967.975163	21.728307
78.414130	2969.065842	21.733325
78.680692	2966.169151	21.738343
78.073801	2973.891555	21.743360
78.331391	2984.906531	21.748378
78.760558	2994.756397	21.753395
78.649112	2997.600712	21.758413
79.055525	2997.305878	21.763431
79.057320	3025.540645	21.768448
79.004261	3018.963091	21.773466
79.160329	3029.859465	21.778483
79.401801	3036.932326	21.783501
79.326586	3019.622494	21.788519
79.455672	3030.606414	21.793536
79.313486	3032.537639	21.798554
79.608838	3043.071560	21.803571
79.685956	3050.566163	21.808589
80.077788	3050.374933	21.813607
79.792791	3063.112231	21.818624
79.786419	3056.550948	21.823642
79.964257	3049.445343	21.828659
79.730921	3067.093016	21.833677
80.415620	3076.703754	21.838695
80.262907	3080.879049	21.843712
80.517734	3075.686836	21.848730
80.758021	3083.602115	21.853747
80.454721	3084.229198	21.858765
80.839578	3069.749685	21.863783
80.855822	3076.410607	21.868800
81.044536	3069.083093	21.873818
80.965638	3078.386770	21.878835
80.770342	3076.005550	21.883853
81.156587	3066.435688	21.888871
81.161300	3075.269967	21.893888
81.303667	3090.356814	21.898906
81.410640	3095.963259	21.903923
81.669229	3099.734598	21.908941
81.823796	3097.931720	21.913959
81.796514	3103.609222	21.918976
81.780349	3098.181533	21.923994
81.953873	3102.714269	21.929011
81.975254	3103.505327	21.934029
81.913763	3096.633440	21.939047
81.920211	3101.882484	21.944064
82.095617	3097.507817	21.949082
82.288607	3097.726710	21.954099
82.381029	3097.014140	21.959117
82.453024	3092.511309	21.964135
82.296344	3093.770078	21.969152
82.414469	3093.636768	21.974170
82.519357	3094.754185	21.979187
82.388295	3109.785923	21.984205
82.642632	3111.716466	21.989223
82.431437	3115.254939	21.994240
82.648486	3128.423773	21.999258
82.520112	3120.259683	22.004275
82.757924	3115.354552	22.009293
82.855421	3119.066342	22.014311
82.635520	3136.113783	22.019328
83.096912	3145.917854	22.024346
83.288946	3143.761885	22.029363
83.171499	3155.695460	22.034381
83.443454	3147.825337	22.039399
83.356908	3161.066519	22.044416
83.448918	3164.804821	22.049434
83.627431	3168.474858	22.054451
83.614449	3173.521612	22.059469
83.963765	3167.962903	22.064487
83.822143	3175.088631	22.069504
84.065678	3171.714962	22.074522
84.496942	3164.385041	22.079539
84.435294	3176.235763	22.084557
84.331301	3171.927420	22.089575
84.589493	3191.925962	22.094592
84.577753	3196.685089	22.099610
84.695018	3203.593143	22.104627
84.171415	3206.206107	22.109645
84.547997	3196.627136	22.114663
84.624925	3202.819358	22.119680
84.564625	3197.966320	22.124698
84.961055	3204.531271	22.129715
84.990529	3219.516057	22.134733
85.479640	3216.974241	22.139751
85.366639	3210.056104	22.144768
85.376332	3213.258783	22.149786
85.521454	3212.701670	22.154803
85.702818	3217.154787	22.159821
85.738602	3212.059435	22.164839
85.708023	3212.852408	22.169856
85.454487	3210.416631	22.174874
85.696300	3227.186519	22.179891
85.456912	3239.330918	22.184909
86.045658	3240.733618	22.189927
85.871005	3253.601240	22.194944
86.215675	3249.669416	22.199962
86.586461	3253.660428	22.204979
86.578532	3274.637485	22.209997
87.071057	3266.931588	22.215015
87.045087	3262.333895	22.220032
86.693930	3256.726558	22.225050
87.030867	3246.984419	22.230067
86.609404	3268.537078	22.235085
87.102174	3263.326667	22.240103
86.882389	3267.441851	22.245120
87.250673	3263.432878	22.250138
87.122476	3262.963545	22.255155
87.147119	3269.012861	22.260173
87.154998	3262.532605	22.265191
87.237411	3259.777781	22.270208
87.535290	3283.398970	22.275226
87.755754	3283.753094	22.280243
87.883271	3287.243396	22.285261
88.045937	3290.070332	22.290279
88.025728	3294.911608	22.295296
87.918511	3298.351795	22.300314
88.329071	3294.676794	22.305331
87.973451	3292.002370	22.310349
88.532044	3292.568644	22.315367
88.143636	3282.838702	22.320384
88.259647	3284.956754	22.325402
88.374852	3285.109782	22.330419
88.435140	3294.524806	22.335437
88.836421	3303.317174	22.340455
88.765883	3311.741563	22.345472
88.948521	3312.994957	22.350490
89.158745	3306.237058	22.355507
88.686875	3316.503675	22.360525
88.976810	3308.180055	22.365543
88.709675	3310.404471	22.370560
88.853709	3314.369258	22.375578
89.279218	3321.196006	22.380595
89.663811	3345.396299	22.385613
89.610149	3333.668568	22.390631
89.394429	3330.981209	22.395648
89.380658	3334.992606	22.400666
89.782496	3325.413706	22.405683
89.723543	3341.147185	22.410701
90.053314	3337.172133	22.415719
90.213301	3355.853544	22.420736
90.015473	3362.392537	22.425754
90.229415	3356.696712	22.430771
90.267598	3366.455633	22.435789
90.135805	3362.506996	22.440807
90.543619	3367.462481	22.445824
90.421386	3363.053551	22.450842
90.647553	3364.973040	22.455859
90.806703	3384.923656	22.460877
90.856751	3383.080566	22.465895
90.860225	3386.462282	22.470912
90.731896	3384.594785	22.475930
90.962687	3385.246053	22.480947
90.999881	3392.997459	22.485965
91.085093	3400.029424	22.490983
91.289970	3412.853233	22.496000
91.326029	3414.674272	22.501018
91.082847	3415.980857	22.506035
91.274860	3432.994671	22.511053
91.495579	3442.851775	22.516071
91.865208	3450.527296	22.521088
91.763014	3451.772346	22.526106
91.987402	3457.664239	22.531123
92.295474	3465.536201	22.536141
92.206172	3473.702337	22.541159
92.916167	3469.289056	22.546176
92.680806	3464.799211	22.551194
93.123064	3458.375310	22.556211
93.275226	3463.100685	22.561229
93.261535	3444.996642	22.566247
93.046824	3441.410966	22.571264
93.012299	3432.879952	22.576282
93.232958	3425.938759	22.581299
93.256282	3433.031385	22.586317
93.352152	3445.909889	22.591335
93.425359	3444.359447	22.596352
93.391921	3452.668701	22.601370
93.305068	3447.561292	22.606387
93.180963	3454.909468	22.611405
93.610473	3446.767412	22.616423
93.263741	3451.646265	22.621440
93.833451	3466.313464	22.626458
93.826075	3469.241037	22.631475
93.833433	3487.456484	22.636493
93.787069	3483.475165	22.641511
93.922846	3480.833921	22.646528
94.146344	3491.267433	22.651546
94.458849	3484.140908	22.656563
94.226208	3497.199454	22.661581
94.293873	3497.034728	22.666599
94.431793	3494.014344	22.671616
94.296605	3508.273043	22.676634
94.740641	3520.836449	22.681651
94.877962	3524.781927	22.686669
95.193174	3529.492531	22.691687
95.195858	3517.178100	22.696704
95.023164	3529.294749	22.701722
95.145078	3527.896489	22.706739
95.198864	3518.478657	22.711757
95.657277	3530.300629	22.716775
95.908045	3548.505768	22.721792
95.486817	3558.195191	22.726810
95.774779	3548.415300	22.731827
96.112545	3550.194274	22.736845
95.778482	3556.907104	22.741863
96.079298	3541.996926	22.746880
96.012519	3549.503783	22.751898
96.064241	3545.444783	22.756915
96.096447	3563.942852	22.761933
96.477946	3581.060508	22.766951
96.566960	3587.118189	22.771968
96.420138	3589.676701	22.776986
96.762214	3574.408831	22.782003
96.654740	3583.649027	22.787021
96.643306	3601.968124	22.792039
97.114422	3605.068099	22.797056
97.034068	3614.974377	22.802074
97.095452	3601.694926	22.807091
97.017519	3603.788829	22.812109
96.827543	3616.269081	22.817127
97.264096	3624.243487	22.822144
97.453330	3629.541586	22.827162
97.834651	3625.896551	22.832179
97.590678	3631.894017	22.837197
97.611752	3655.465527	22.842215
98.110855	3657.604461	22.847232
98.276053	3659.478171	22.852250
98.054923	3663.695267	22.857267
98.368014	3658.879879	22.862285
98.612214	3648.793747	22.867303
98.692827	3655.149339	22.872320
98.405837	3667.671682	22.877338
98.879325	3676.748013	22.882355
99.207235	3684.544351	22.887373
99.070458	3686.861422	22.892391
99.219259	3686.485991	22.897408
98.892282	3695.204260	22.902426
99.347122	3685.043065	22.907443
99.408676	3676.607441	22.912461
99.323524	3679.118744	22.917479
99.320308	3682.754813	22.922496
99.447840	3701.218754	22.927514
99.717712	3702.600668	22.932531
99.964613	3710.101339	22.937549
100.092698	3713.383348	22.942567
100.173823	3706.851798	22.947584
100.230906	3712.204882	22.952602
100.157845	3712.651720	22.957619
100.187255	3703.511864	22.962637
100.000444	3715.653832	22.967655
100.465108	3727.269774	22.972672
100.465115	3732.716972	22.977690
100.397845	3741.283982	22.982707
100.370847	3744.933454	22.987725
100.757565	3754.797526	22.992743
100.854644	3751.507835	22.997760
100.988355	3767.623281	23.002778
101.354800	3758.797715	23.007795
101.407923	3761.862590	23.012813
101.416813	3754.807477	23.017831
101.637250	3752.681374	23.022848
101.451651	3749.277444	23.027866
101.705105	3753.545134	23.032883
101.976988	3767.824473	23.037901
102.067056	3782.809217	23.042919
101.991019	3787.445294	23.047936
102.200448	3786.060870	23.052954
102.335778	3785.382116	23.057971
102.315504	3790.318450	23.062989
102.288334	3791.360527	23.068007
102.518113	3783.051344	23.073024
102.363699	3784.672831	23.078042
102.514074	3800.404793	23.083059
102.727206	3809.986577	23.088077
102.619971	3819.815928	23.093095
102.814898	3816.179269	23.098112
102.946902	3821.495966	23.103130
102.667097	3826.627274	23.108147
102.888234	3838.743527	23.113165
102.901335	3853.359140	23.118183
103.208931	3848.593823	23.123200
103.387166	3869.612516	23.128218
103.760367	3877.653457	23.133235
104.128747	3870.686821	23.138253
103.616699	3871.318963	23.143271
103.739156	3871.337314	23.148288
103.858886	3893.658425	23.153306
104.025380	3899.315549	23.158323
104.066011	3897.720843	23.163341
104.082417	3904.459661	23.168359
104.503684	3914.268107	23.173376
104.829850	3924.086794	23.178394
104.760241	3923.125386	23.183411
105.026516	3920.727460	23.188429
104.928464	3927.796701	23.193447
105.388422	3911.180844	23.198464
105.573831	3916.869493	23.203482
105.575000	3914.818262	23.208499
105.833494	3904.766613	23.213517
105.527149	3917.906225	23.218535
106.068852	3903.670093	23.223552
105.736789	3906.685372	23.228570
105.916579	3921.844789	23.233587
106.154977	3922.797227	23.238605
105.928482	3936.721384	23.243623
106.641641	3925.371431	23.248640
106.423836	3939.198075	23.253658
106.508126	3926.919423	23.258675
106.481153	3921.605459	23.263693
106.461973	3935.404331	23.268711
106.646188	3927.284531	23.273728
106.334611	3944.842587	23.278746
106.682583	3949.679804	23.283763
106.851833	3954.671042	23.288781
106.933738	3964.815673	23.293799
106.923343	3974.547972	23.298816
107.310179	3984.574006	23.303834
107.452063	3989.272105	23.308851
107.549310	3984.457706	23.313869
107.409782	3991.570463	23.318887
107.765500	3981.167579	23.323904
107.782528	4003.860234	23.328922
107.868904	4012.966996	23.333939
108.067499	4020.358869	23.338957
108.365065	4028.256482	23.343975
108.208328	4015.856228	23.348992
108.226291	4021.831340	23.354010
108.198431	4014.354574	23.359027
108.459526	4021.725073	23.364045
108.452045	4046.806453	23.369063
108.796058	4043.940451	23.374080
108.635003	4044.457782	23.379098
108.789315	4042.122477	23.384115
108.879847	4052.902839	23.389133
108.936499	4071.026144	23.394151
109.110871	4068.898569	23.399168
109.205112	4081.392769	23.404186
108.997963	4082.892683	23.409203
109.263812	4098.364449	23.414221
109.406833	4113.454932	23.419239
109.803555	4108.512944	23.424256
110.096809	4120.397756	23.429274
109.919236	4134.782958	23.434291
110.317070	4129.751790	23.439309
110.424393	4135.494793	23.444327
110.209747	4122.849672	23.449344
110.406178	4132.569087	23.454362
110.239714	4142.554138	23.459379
110.859651	4150.385836	23.464397
110.833050	4164.908297	23.469415
110.820277	4171.230341	23.474432
110.775034	4156.299310	23.479450
110.999349	4176.049564	23.484467
111.260172	4184.477045	23.489485
111.503673	4194.924254	23.494503
111.762800	4179.781360	23.499520
111.524520	4191.467576	23.504538
111.654136	4202.007674	23.509555
111.792400	4215.064860	23.514573
111.794568	4226.163958	23.519591
111.909309	4215.569287	23.524608
112.208911	4218.160299	23.529626
112.208984	4225.102385	23.534643
112.358755	4238.257701	23.539661
112.218301	4247.723468	23.544679
112.868193	4250.027315	23.549696
112.837457	4240.210381	23.554714
112.825758	4247.456837	23.559731
113.373296	4255.336014	23.564749
113.286240	4270.283611	23.569767
113.464728	4260.014630	23.574784
113.403165	4273.634959	23.579802
113.450079	4266.667037	23.584819
113.796616	4259.037598	23.589837
113.729368	4266.606697	23.594855
113.898379	4260.496657	23.599872
114.076168	4257.024966	23.604890
114.100962	4284.209598	23.609907
114.495404	4284.014385	23.614925
114.223738	4296.229127	23.619943
114.560790	4286.396156	23.624960
114.756769	4284.693393	23.629978
114.408454	4283.934434	23.634995
114.877544	4279.024514	23.640013
114.800241	4288.119948	23.645031
115.089471	4306.116812	23.650048
115.304954	4309.610891	23.655066
114.955245	4313.194616	23.660083
115.379965	4311.118487	23.665101
115.524297	4309.248653	23.670119
115.351092	4317.007789	23.675136
115.337665	4316.350887	23.680154
115.288701	4333.194915	23.685171
115.783896	4332.408907	23.690189
115.626361	4342.566652	23.695207
116.031591	4336.551352	23.700224
116.091445	4348.233210	23.705242
115.995180	4365.975019	23.710259
116.130946	4367.839513	23.715277
116.290751	4372.493415	23.720295
116.090952	4380.058527	23.725312
116.639708	4382.602801	23.730330
116.584721	4404.110116	23.735347
116.733535	4400.870002	23.740365
116.684698	4407.639920	23.745383
116.817026	4428.740599	23.750400
117.278018	4425.589761	23.755418
117.325523	4432.712306	23.760435
117.542516	4428.504038	23.765453
117.644138	4441.936048	23.770471
117.457426	4448.160209	23.775488
117.986408	4444.329489	23.780506
118.219333	4458.382404	23.785523
118.366726	4441.677168	23.790541
118.262157	4457.972959	23.795559
118.399224	4467.433073	23.800576
118.663672	4467.835074	23.805594
118.786252	4482.031500	23.810611
119.023225	4474.331105	23.815629
118.816076	4472.626554	23.820647
119.026508	4475.491475	23.825664
119.255277	4473.847840	23.830682
119.195727	4493.341505	23.835699
119.446209	4489.402528	23.840717
119.639419	4500.830094	23.845735
119.492082	4500.312700	23.850752
119.845832	4496.437740	23.855770
119.289699	4500.669967	23.860787
119.935155	4521.213285	23.865805
119.852038	4529.870372	23.870823
119.706850	4536.297179	23.875840
120.150711	4551.144536	23.880858
120.514510	4556.593213	23.885875
120.319927	4560.393085	23.890893
120.680742	4564.943671	23.895911
120.677771	4566.933541	23.900928
121.297253	4579.659339	23.905946
120.783456	4588.916211	23.910963
121.247748	4588.114833	23.915981
121.428442	4592.050250	23.920999
121.307973	4594.177710	23.926016
121.610891	4601.014690	23.931034
121.595741	4618.589782	23.936051
121.620255	4607.946782	23.941069
121.979402	4619.172912	23.946087
121.367267	4618.982125	23.951104
121.872847	4632.456094	23.956122
122.311220	4647.020146	23.961139
122.515142	4645.728705	23.966157
122.706635	4649.562329	23.971175
122.571611	4650.468355	23.976192
122.600691	4660.324488	23.981210
122.618089	4677.360298	23.986227
122.724885	4664.467780	23.991245
123.038254	4667.270803	23.996263
123.293118	4684.438200	24.001280
123.484586	4694.047741	24.006298
123.421841	4701.165823	24.011315
123.358031	4691.725807	24.016333
123.704828	4694.891087	24.021351
123.911872	4715.971118	24.026368
124.300058	4718.275055	24.031386
123.942009	4727.771625	24.036403
124.091814	4723.995745	24.041421
124.463891	4721.378568	24.046439
124.244726	4731.811385	24.051456
124.618362	4725.238857	24.056474
124.855190	4742.319523	24.061491
124.729802	4753.489729	24.066509
124.968402	4765.016292	24.071527
125.004993	4761.898643	24.076544
125.517054	4755.050378	24.081562
125.156785	4757.385314	24.086579
125.393783	4756.037984	24.091597
125.543046	4758.824092	24.096615
125.566076	4771.151856	24.101632
125.451384	4781.737520	24.106650
125.764574	4782.906415	24.111667
126.116202	4792.469021	24.116685
126.206669	4811.653145	24.121703
126.157849	4811.698283	24.126720
126.477315	4804.955128	24.131738
126.446692	4814.409350	24.136755
126.162219	4818.264332	24.141773
126.571745	4831.920552	24.146791
126.280714	4840.610660	24.151808
126.660994	4858.091407	24.156826
127.106847	4876.963174	24.161843
127.288537	4872.383392	24.166861
127.592474	4876.739509	24.171879
127.671864	4886.565403	24.176896
128.023702	4890.075627	24.181914
128.095938	4899.902713	24.186931
128.014400	4902.016681	24.191949
128.293664	4908.686811	24.196967
128.257668	4902.371836	24.201984
128.261141	4893.961716	24.207002
128.244495	4916.351752	24.212019
128.652901	4922.149151	24.217037
128.891444	4922.293984	24.222055
128.624656	4917.838061	24.227072
128.532968	4926.084102	24.232090
129.005206	4946.433778	24.237107
129.078123	4954.910113	24.242125
129.365157	4956.187311	24.247143
129.484010	4984.012045	24.252160
129.870513	4980.597785	24.257178
129.762865	4989.751414	24.262195
130.077048	4991.660474	24.267213
130.238980	4977.170838	24.272231
130.056153	4995.979089	24.277248
130.518360	5004.752488	24.282266
130.522489	5009.375651	24.287283
130.759898	5009.010329	24.292301
130.712735	5008.456642	24.297319
130.744907	5008.847500	24.302336
131.117173	5021.587814	24.307354
131.098115	5039.344376	24.312371
131.208868	5053.620458	24.317389
131.569711	5046.368668	24.322407
131.365390	5051.513862	24.327424
131.306290	5048.960148	24.332442
131.515535	5066.719893	24.337459
131.907719	5073.833702	24.342477
132.148426	5074.852382	24.347495
131.850118	5077.655159	24.352512
132.557744	5088.884571	24.357530
132.385825	5102.640449	24.362547
132.577423	5114.302638	24.367565
132.947383	5099.935961	24.372583
132.650811	5102.339944	24.377600
133.052761	5098.486786	24.382618
133.226371	5103.290621	24.387635
133.206613	5116.687388	24.392653
133.544458	5120.057431	24.397671
133.510434	5126.692893	24.402688
133.408627	5121.892992	24.407706
133.838379	5125.017060	24.412723
133.760964	5125.024404	24.417741
133.884260	5141.979389	24.422759
133.721430	5150.887862	24.427776
133.959687	5159.766947	24.432794
134.029030	5164.735342	24.437811
134.192736	5176.256494	24.442829
134.491546	5182.980211	24.447847
134.507661	5198.774002	24.452864
134.655799	5196.581315	24.457882
135.025449	5211.068274	24.462899
135.142120	5214.151263	24.467917
135.360891	5212.702954	24.472935
135.394033	5219.915655	24.477952
135.617564	5222.097291	24.482970
135.370973	5230.703071	24.487987
135.576077	5230.514785	24.493005
136.074602	5238.167093	24.498023
135.902067	5261.138672	24.503040
136.005537	5258.080734	24.508058
136.069003	5267.808691	24.513075
136.135627	5275.941281	24.518093
136.627213	5283.906642	24.523111
136.757922	5294.097606	24.528128
137.017303	5292.975713	24.533146
137.168076	5309.112756	24.538163
137.085050	5321.764880	24.543181
136.992937	5318.852725	24.548199
137.350021	5333.256819	24.553216
137.450880	5345.313030	24.558234
137.811966	5346.003065	24.563251
138.146992	5346.644645	24.568269
138.109886	5342.964935	24.573287
138.278619	5368.875349	24.578304
138.189621	5370.488134	24.583322
138.403363	5383.362888	24.588339
138.557989	5386.330941	24.593357
138.942219	5389.899711	24.598375
138.685581	5401.604824	24.603392
139.345854	5409.699049	24.608410
139.387225	5403.488415	24.613427
139.165064	5407.910522	24.618445
139.665603	5398.816904	24.623463
139.343396	5426.971412	24.628480
139.663068	5433.024695	24.633498
139.792165	5439.922326	24.638515
139.606142	5439.327032	24.643533
139.802199	5449.029210	24.648551
140.035204	5469.386096	24.653568
140.302657	5472.941141	24.658586
140.430008	5485.034816	24.663603
140.335366	5498.704209	24.668621
140.860781	5496.244242	24.673639
140.810719	5512.830595	24.678656
140.759640	5515.654734	24.683674
140.968873	5524.205680	24.688691
141.077243	5536.684520	24.693709
141.565797	5552.773763	24.698727
142.100823	5558.075516	24.703744
141.984308	5562.797575	24.708762
142.121733	5549.746470	24.713779
141.765633	5563.884510	24.718797
142.188934	5574.265853	24.723815
142.477599	5579.483175	24.728832
142.819977	5576.651040	24.733850
143.005602	5577.933267	24.738867
142.706738	5584.737999	24.743885
142.994144	5581.660570	24.748903
142.861322	5584.307658	24.753920
143.208513	5604.155140	24.758938
143.452648	5606.063273	24.763955
143.513565	5607.860762	24.768973
143.425347	5602.229911	24.773991
143.612841	5630.653234	24.779008
143.856211	5632.125168	24.784026
143.926738	5630.204391	24.789043
144.100191	5647.061041	24.794061
144.401053	5651.339913	24.799079
144.603514	5665.695877	24.804096
144.553114	5658.878920	24.809114
144.768092	5662.241071	24.814131
144.665419	5681.381047	24.819149
145.345257	5680.274574	24.824167
145.375416	5688.184223	24.829184
145.222402	5686.666685	24.834202
145.525029	5696.564024	24.839219
145.554096	5719.839984	24.844237
145.543335	5719.922140	24.849255
145.660657	5723.624178	24.854272
145.942295	5737.902516	24.859290
145.930642	5746.351536	24.864307
145.914399	5755.696827	24.869325
146.488580	5770.245738	24.874343
146.415520	5781.182750	24.879360
146.763739	5778.441763	24.884378
146.841575	5799.246135	24.889395
147.420732	5813.276804	24.894413
147.825329	5806.104063	24.899431
147.278493	5812.050500	24.904448
147.491145	5818.941551	24.909466
147.560029	5832.585734	24.914483
147.353106	5826.975244	24.919501
147.975187	5838.785652	24.924519
148.116786	5857.998025	24.929536
148.397538	5859.596897	24.934554
148.810495	5856.343471	24.939571
148.632696	5864.634974	24.944589
148.785862	5877.481569	24.949607
149.377503	5899.391871	24.954624
149.299405	5885.117570	24.959642
149.463738	5887.105110	24.964659
149.351030	5893.385320	24.969677
149.635768	5898.194628	24.974695
149.688789	5912.917384	24.979712
149.971765	5916.571563	24.984730
150.219183	5910.968519	24.989747
149.854489	5923.114854	24.994765
149.964083	5926.733157	24.999783
150.264326	5947.908097	25.004800
150.396513	5949.181088	25.009818
150.671058	5963.697877	25.014835
150.132306	5987.033587	25.019853
150.864422	5979.452902	25.024871
150.773068	6000.248532	25.029888
150.797455	6013.715936	25.034906
151.118377	6011.215714	25.039923
151.319234	6035.029204	25.044941
151.399042	6035.312961	25.049959
151.985284	6059.359613	25.054976
152.035479	6075.176204	25.059994
152.024486	6072.739590	25.065011
152.277949	6072.968606	25.070029
152.345235	6067.673361	25.075047
152.667631	6089.726957	25.080064
153.014931	6099.558082	25.085082
153.288293	6090.683625	25.090099
153.018317	6099.926995	25.095117
153.389654	6103.311398	25.100135
153.635160	6106.352754	25.105152
153.520437	6121.101901	25.110170
154.187638	6122.298928	25.115187
153.847514	6128.454632	25.120205
154.198794	6126.200618	25.125223
154.163305	6121.339812	25.130240
154.354800	6138.299540	25.135258
154.510055	6136.829373	25.140275
154.826812	6151.492145	25.145293
154.453369	6149.139158	25.150311
154.951087	6166.071845	25.155328
154.707255	6171.410608	25.160346
155.138954	6173.901318	25.165363
154.888097	6194.985104	25.170381
155.167362	6195.666673	25.175399
155.831905	6211.741630	25.180416
155.689504	6230.799845	25.185434
156.173051	6234.453184	25.190451
156.347731	6241.180579	25.195469
156.335843	6249.665350	25.200487
156.822256	6257.907735	25.205504
156.478000	6268.722219	25.210522
157.087489	6269.371172	25.215539
156.882650	6272.383155	25.220557
157.115223	6289.926180	25.225575
157.358870	6289.096674	25.230592
157.382440	6299.020903	25.235610
157.836864	6303.122516	25.240627
157.859225	6312.009643	25.245645
158.102782	6317.696233	25.250663
158.165330	6316.394199	25.255680
158.288906	6336.143365	25.260698
158.860765	6331.957757	25.265715
158.850370	6348.702245	25.270733
158.905859	6352.995155	25.275751
159.195240	6351.112883	25.280768
159.309435	6357.973213	25.285786
159.398119	6360.119839	25.290803
159.522014	6374.924231	25.295821
159.275551	6382.325530	25.300839
159.459903	6382.376173	25.305856
159.595303	6400.155160	25.310874
159.979050	6412.501671	25.315891
159.976529	6416.997962	25.320909
159.915149	6425.535916	25.325927
160.232508	6435.794382	25.330944
160.160282	6454.706561	25.335962
160.544605	6468.095067	25.340979
160.693159	6484.122622	25.345997
160.834177	6489.246547	25.351015
160.984690	6499.435011	25.356032
161.348517	6515.183574	25.361050
161.721048	6519.657968	25.366067
161.757799	6532.253421	25.371085
161.917469	6548.020853	25.376103
162.256235	6543.069598	25.381120
162.214919	6561.702687	25.386138
162.403676	6567.519737	25.391155
162.554606	6573.571469	25.396173
162.796618	6571.086589	25.401191
162.789727	6572.956851	25.406208
163.098772	6601.240496	25.411226
163.331556	6602.533117	25.416243
163.368299	6610.995852	25.421261
163.510758	6605.969172	25.426279
163.707263	6611.209186	25.431296
163.561285	6624.516279	25.436314
163.627334	6621.102745	25.441331
164.302660	6634.923679	25.446349
163.875526	6650.110988	25.451367
164.194834	6656.152991	25.456384
164.269369	6670.493242	25.461402
164.125117	6687.561919	25.466419
164.393633	6696.581003	25.471437
164.756051	6722.128391	25.476455
164.862792	6721.794909	25.481472
164.735922	6741.225300	25.486490
165.621967	6747.652400	25.491507
165.597509	6772.312436	25.496525
165.680738	6779.540397	25.501543
166.158537	6782.381169	25.506560
166.344415	6800.858775	25.511578
166.667333	6803.670058	25.516595
166.710428	6810.481707	25.521613
166.576629	6820.957685	25.526631
167.577266	6829.162493	25.531648
167.312179	6834.789341	25.536666
167.612841	6836.885183	25.541683
167.788338	6832.508293	25.546701
167.339747	6842.245594	25.551719
167.486397	6848.411563	25.556736
167.582092	6881.397123	25.561754
167.922604	6888.488019	25.566771
168.072212	6895.912986	25.571789
168.387111	6914.386691	25.576807
168.813777	6924.558064	25.581824
168.871064	6932.509527	25.586842
168.800579	6932.514934	25.591859
168.839010	6958.831542	25.596877
169.265475	6973.135067	25.601895
169.590677	6981.424215	25.606912
169.427595	6995.128283	25.611930
169.849589	6996.117866	25.616947
169.759909	7011.175608	25.621965
169.849614	7025.496340	25.626983
170.279795	7030.029075	25.632000
170.490179	7052.520811	25.637018
170.928468	7057.527176	25.642035
170.883604	7054.747082	25.647053
170.826402	7069.385188	25.652071
170.979509	7083.311879	25.657088
171.350511	7097.471103	25.662106
171.360878	7105.082270	25.667123
172.096398	7108.430228	25.672141
171.967583	7119.320680	25.677159
172.069384	7114.996873	25.682176
172.208361	7133.114788	25.687194
172.395888	7138.580950	25.692212
172.655058	7146.154883	25.697229
172.767461	7169.457769	25.702247
173.220765	7169.262244	25.707264
173.210389	7173.222854	25.712282
173.456993	7174.965362	25.717300
173.691398	7199.336660	25.722317
173.573916	7214.101455	25.727335
173.846796	7206.326843	25.732352
173.732051	7210.248818	25.737370
174.150658	7227.230400	25.742388
174.521111	7235.854041	25.747405
174.199967	7244.440168	25.752423
174.670024	7242.785452	25.757440
174.506639	7262.681740	25.762458
174.606511	7267.980505	25.767476
174.937486	7276.466560	25.772493
174.828670	7297.553494	25.777511
175.169178	7304.672147	25.782528
175.194695	7336.208332	25.787546
175.537714	7333.464007	25.792564
175.777593	7347.633348	25.797581
175.687994	7370.535171	25.802599
176.395590	7377.953053	25.807616
176.420731	7398.897428	25.812634
176.606854	7395.974269	25.817652
177.198768	7403.594847	25.822669
177.318990	7425.260001	25.827687
177.369345	7433.832772	25.832704
177.649107	7429.673976	25.837722
177.393924	7436.215475	25.842740
177.624185	7443.913277	25.847757
177.500884	7461.749674	25.852775
177.872691	7466.421382	25.857792
177.876634	7485.998013	25.862810
178.180509	7507.173649	25.867828
179.096170	7514.121556	25.872845
178.580052	7525.670326	25.877863
179.013521	7544.708815	25.882880
179.165188	7550.625316	25.887898
179.211893	7557.075924	25.892916
179.728491	7565.928400	25.897933
179.821626	7578.250681	25.902951
180.361204	7586.413282	25.907968
180.222625	7584.980603	25.912986
180.466011	7601.819091	25.918004
180.731578	7603.229250	25.923021
180.506547	7605.857278	25.928039
181.006620	7630.505845	25.933056
181.253001	7635.792293	25.938074
180.994851	7639.805068	25.943092
181.392750	7650.559842	25.948109
181.502296	7668.953421	25.953127
181.868149	7668.306841	25.958144
182.254063	7688.293889	25.963162
182.251446	7690.703150	25.968180
182.567627	7693.245528	25.973197
182.444210	7709.978653	25.978215
182.909101	7716.824835	25.983232
183.012879	7719.721402	25.988250
182.878087	7720.520431	25.993268
183.362841	7742.558901	25.998285
182.987226	7758.386224	26.003303
183.494065	7765.461793	26.008320
183.669398	7784.321174	26.013338
183.815614	7796.270128	26.018356
184.613412	7797.510268	26.023373
184.207711	7819.372521	26.028391
184.260568	7818.098752	26.033408
184.517971	7833.482633	26.038426
184.880070	7861.177623	26.043444
185.236528	7853.410917	26.048461
185.259993	7876.260088	26.053479
185.225202	7882.130386	26.058496
185.614357	7884.462211	26.063514
186.022014	7898.309664	26.068532
186.274524	7912.500262	26.073549
186.159654	7912.132553	26.078567
186.474536	7918.886289	26.083584
186.474159	7939.269233	26.088602
186.422203	7947.229048	26.093620
186.992425	7954.918866	26.098637
186.886877	7963.707572	26.103655
187.098157	7967.335502	26.108672
187.100823	7987.893665	26.113690
187.170794	8003.745136	26.118708
187.757536	8005.544855	26.123725
187.548487	8026.359466	26.128743
187.856863	8033.727173	26.133760
188.106271	8049.432399	26.138778
188.270589	8070.956431	26.143796
188.573719	8076.068997	26.148813
189.085579	8093.741077	26.153831
189.400464	8093.802417	26.158848
189.323940	8106.770767	26.163866
189.526444	8123.701649	26.168884
189.634856	8125.961832	26.173901
189.934371	8138.627697	26.178919
190.165158	8155.602770	26.183936
190.271137	8159.158377	26.188954
190.394389	8166.681254	26.193972
190.597596	8172.182988	26.198989
190.468760	8189.143588	26.204007
190.879294	8205.187797	26.209024
190.766365	8217.821968	26.214042
191.300362	8245.019681	26.219060
191.547308	8253.141275	26.224077
191.479859	8256.186810	26.229095
191.572956	8281.813591	26.234112
191.617963	8292.119139	26.239130
191.794743	8321.078407	26.244148
192.338871	8324.002223	26.249165
192.514972	8351.281426	26.254183
192.993706	8354.259400	26.259200
193.412560	8376.684621	26.264218
193.211820	8392.075569	26.269236
193.751747	8397.066324	26.274253
193.796593	8410.007738	26.279271
193.403289	8425.332131	26.284288
194.440419	8434.469942	26.289306
194.279191	8444.690783	26.294324
194.685832	8451.498876	26.299341
194.659544	8460.430705	26.304359
194.929636	8475.431052	26.309376
195.167402	8475.305076	26.314394
195.359899	8497.840414	26.319412
195.807973	8511.722673	26.324429
195.853033	8516.527562	26.329447
196.081553	8544.445941	26.334464
196.330648	8540.391980	26.339482
196.265311	8547.410594	26.344500
196.734584	8552.780972	26.349517
196.826405	8573.648102	26.354535
197.057478	8574.734784	26.359552
197.187451	8578.462180	26.364570
197.156118	8605.721805	26.369588
197.893898	8595.775729	26.374605
197.868440	8602.811397	26.379623
197.887913	8624.855647	26.384640
198.026426	8620.427677	26.389658
198.367448	8649.009013	26.394676
198.349877	8651.431135	26.399693
198.532292	8662.775269	26.404711
198.949109	8677.942939	26.409728
198.974188	8687.665168	26.414746
199.303609	8697.626121	26.419764
199.775945	8703.950009	26.424781
199.746525	8729.427637	26.429799
199.689333	8727.292885	26.434816
200.036541	8726.412241	26.439834
200.614947	8741.709983	26.444852
200.548224	8747.636301	26.449869
200.673705	8755.463947	26.454887
200.921037	8763.340746	26.459904
200.909350	8773.592970	26.464922
201.220625	8786.333816	26.469940
201.318014	8791.274284	26.474957
201.266778	8808.500770	26.479975
201.488042	8816.325980	26.484992
201.774981	8838.193113	26.490010
201.502915	8857.819482	26.495028
202.221358	8874.171033	26.500045
202.062949	8886.488702	26.505063
202.199460	8910.615711	26.510080
203.025716	8925.967129	26.515098
203.186581	8941.424780	26.520116
203.265611	8948.666238	26.525133
203.617702	8966.554014	26.530151
203.572543	8982.067870	26.535168
203.721714	9005.675366	26.540186
204.158019	9026.901208	26.545204
204.170864	9033.473032	26.550221
204.563636	9039.004341	26.555239
204.743965	9057.826586	26.560256
205.452825	9066.231346	26.565274
205.453925	9074.173484	26.570292
205.775137	9079.526802	26.575309
206.094419	9087.805429	26.580327
205.922333	9094.685976	26.585344
206.325925	9102.809642	26.590362
206.451733	9123.065279	26.595380
206.514410	9120.638060	26.600397
206.788612	9139.967941	26.605415
206.495049	9159.141329	26.610432
207.004163	9166.867064	26.615450
207.014917	9184.421645	26.620468
207.651237	9202.276810	26.625485
207.929193	9215.921578	26.630503
207.959871	9225.776341	26.635520
208.417280	9249.492297	26.640538
208.083968	9259.670457	26.645556
208.573897	9266.807796	26.650573
208.921220	9282.209699	26.655591
209.056113	9294.923432	26.660608
209.243181	9319.809196	26.665626
209.181703	9327.035486	26.670644
209.488947	9343.515465	26.675661
210.131933	9348.574543	26.680679
210.095516	9369.500966	26.685696
210.254404	9373.451430	26.690714
210.553215	9386.605254	26.695732
210.623111	9400.036472	26.700749
210.980556	9411.750781	26.705767
210.728823	9429.095418	26.710784
211.588267	9435.694260	26.715802
211.421111	9453.117880	26.720820
211.523907	9472.203965	26.725837
212.127434	9476.774097	26.730855
212.101529	9501.709583	26.735872
212.455534	9508.114043	26.740890
212.537836	9521.888361	26.745908
212.881868	9540.693526	26.750925
213.097517	9553.383853	26.755943
213.284425	9563.209019	26.760960
213.343669	9571.090571	26.765978
213.479607	9579.517187	26.770996
213.806558	9594.220840	26.776013
214.057914	9601.933526	26.781031
214.244727	9610.470693	26.786048
214.880692	9625.238234	26.791066
214.608479	9641.387465	26.796084
215.052817	9640.757759	26.801101
215.241466	9655.763244	26.806119
215.096286	9671.624412	26.811136
215.568387	9670.557608	26.816154
215.389231	9702.490000	26.821172
215.666858	9702.938028	26.826189
216.200591	9718.860951	26.831207
216.125373	9736.054587	26.836224
216.307839	9761.069422	26.841242
216.650913	9779.265266	26.846260
216.486052	9789.217346	26.851277
217.208054	9811.601484	26.856295
216.888016	9839.918602	26.861312
217.656076	9846.747030	26.866330
217.498077	9866.397498	26.871348
217.545974	9882.223757	26.876365
218.026589	9904.633019	26.881383
218.485589	9932.202110	26.886400
218.553781	9943.596787	26.891418
218.544913	9953.403396	26.896436
219.120570	9965.629514	26.901453
219.461575	9977.878732	26.906471
219.386468	10006.067358	26.911488
219.737879	10008.132381	26.916506
220.147168	10033.992442	26.921524
220.486275	10058.851031	26.926541
220.885892	10060.610285	26.931559
220.944592	10073.148959	26.936576
221.210601	10085.951119	26.941594
221.442741	10092.651725	26.946612
221.478964	10107.029764	26.951629
222.011938	10116.316621	26.956647
222.110094	10126.174157	26.961664
222.510741	10144.721707	26.966682
222.552125	10152.714432	26.971700
222.637144	10157.755847	26.976717
222.590360	10171.578878	26.981735
223.002409	10183.220111	26.986752
223.373273	10202.555754	26.991770
223.477701	10214.875832	26.996788
223.801191	10228.953532	27.001805
224.287583	10238.012611	27.006823
224.143446	10258.023660	27.011840
224.309364	10267.613234	27.016858
224.791600	10281.058072	27.021876
225.119722	10302.796696	27.026893
225.215070	10300.641995	27.031911
225.189408	10324.410364	27.036928
225.681900	10336.196745	27.041946
225.887272	10343.111451	27.046964
226.011914	10363.563439	27.051981
226.520338	10361.422280	27.056999
226.199797	10389.837348	27.062016
226.506332	10404.094483	27.067034
226.869905	10417.741858	27.072052
226.561712	10437.018452	27.077069
227.198919	10447.904097	27.082087
227.209010	10475.080462	27.087104
227.393450	10482.769986	27.092122
228.096733	10499.135956	27.097140
227.946068	10524.408025	27.102157
228.533638	10531.076761	27.107175
228.637663	10544.808967	27.112192
229.027454	10553.670714	27.117210
229.144294	10562.981026	27.122228
229.155451	10579.610561	27.127245
229.532703	10598.382315	27.132263
229.706584	10614.735989	27.137280
229.944367	10616.573308	27.142298
230.303608	10630.257034	27.147316
230.273139	10641.689021	27.152333
230.543375	10654.171069	27.157351
230.537200	10671.063556	27.162368
231.198858	10690.544668	27.167386
231.504705	10712.556977	27.172404
231.547361	10725.325716	27.177421
231.709331	10727.988659	27.182439
231.544076	10752.073847	27.187456
232.227124	10762.280081	27.192474
232.346655	10795.748770	27.197492
232.526524	10806.544133	27.202509
233.005813	10819.068911	27.207527
232.908565	10843.631446	27.212544
233.107082	10858.553694	27.217562
233.767297	10877.685465	27.222580
233.636233	10887.607413	27.227597
234.261054	10913.473388	27.232615
234.254121	10932.630580	27.237632
234.480408	10943.921005	27.242650
234.753838	10965.611277	27.247668
234.925305	10988.821698	27.252685
235.493666	10991.934246	27.257703
235.604767	11020.315206	27.262720
235.956596	11028.179761	27.267738
236.385848	11051.771468	27.272756
236.415594	11062.251497	27.277773
236.500320	11069.501635	27.282791
236.872318	11090.676250	27.287808
237.328616	11109.662421	27.292826
237.290866	11121.915336	27.297844
237.473977	11137.377719	27.302861
238.216775	11149.769315	27.307879
238.058379	11153.244871	27.312896
238.026232	11171.045079	27.317914
238.669946	11185.859264	27.322932
238.586670	11207.432428	27.327949
238.907742	11223.466111	27.332967
238.866360	11236.277529	27.337984
239.657626	11245.908343	27.343002
239.794974	11267.385185	27.348020
239.942353	11283.713984	27.353037
240.067803	11304.395514	27.358055
240.469590	11324.155203	27.363072
240.625796	11329.504292	27.368090
240.925319	11345.971846	27.373108
240.994464	11370.613210	27.378125
241.555456	11384.443816	27.383143
241.902891	11399.305670	27.388160
241.819823	11407.481922	27.393178
242.091871	11419.480503	27.398196
241.991325	11448.555921	27.403213
242.371581	11464.097860	27.408231
242.538386	11490.875743	27.413248
242.712563	11503.293986	27.418266
243.098780	11510.286409	27.423284
243.281228	11538.568223	27.428301
243.822580	11549.784855	27.433319
243.768458	11567.701016	27.438336
244.288720	11580.088815	27.443354
244.423255	11603.282595	27.448372
244.675059	11622.353647	27.453389
245.105443	11626.559123	27.458407
245.448473	11639.652319	27.463424
244.952818	11655.456053	27.468442
245.848081	11668.196273	27.473460
245.688349	11683.893999	27.478477
246.237222	11701.913764	27.483495
246.105728	11725.235275	27.488512
246.621153	11737.464840	27.493530
246.648248	11744.627121	27.498548
246.592716	11775.525174	27.503565
247.371648	11792.733238	27.508583
247.846706	11812.851709	27.513600
247.561069	11822.940063	27.518618
248.277447	11840.336599	27.523636
248.086134	11857.938569	27.528653
248.485973	11872.385625	27.533671
248.860973	11898.627033	27.538688
248.763899	11912.704127	27.543706
249.631912	11938.370755	27.548724
249.438280	11947.678108	27.553741
250.048500	11968.163625	27.558759
250.516175	11979.220989	27.563776
250.679171	11993.437895	27.568794
250.943424	12012.964336	27.573812
250.990584	12014.133709	27.578829
251.522448	12035.777907	27.583847
251.357554	12049.398325	27.588864
251.610454	12069.695718	27.593882
252.322158	12075.537728	27.598900
252.196518	12099.553748	27.603917
252.596202	12105.956416	27.608935
252.584023	12127.797956	27.613952
252.879729	12143.861965	27.618970
253.179727	12169.536321	27.623988
253.599372	12178.721797	27.629005
253.753154	12192.707179	27.634023
253.863561	12207.484523	27.639040
254.012809	12227.542409	27.644058
254.664442	12242.258555	27.649076
254.725757	12268.883418	27.654093
255.078867	12277.742734	27.659111
255.255166	12300.527180	27.664128
255.433322	12320.975935	27.669146
255.697790	12321.683876	27.674164
256.302132	12351.748895	27.679181
256.438904	12371.410333	27.684199
256.457954	12385.021068	27.689216
256.788559	12389.537949	27.694234
257.344882	12405.581137	27.699252
257.222250	12443.538824	27.704269
257.282544	12444.592592	27.709287
258.224939	12457.495831	27.714304
258.235430	12488.860222	27.719322
258.714008	12491.729491	27.724340
258.691884	12515.238892	27.729357
259.044287	12530.606819	27.734375
259.186658	12546.414529	27.739392
258.967070	12557.861839	27.744410
259.156942	12575.243894	27.749428
259.653180	12595.550514	27.754445
260.137235	12619.800459	27.759463
260.642941	12637.253217	27.764480
260.781258	12656.174077	27.769498
261.165718	12670.838712	27.774516
261.501303	12697.817575	27.779533
261.580851	12701.447905	27.784551
261.634710	12710.976321	27.789568
261.822420	12733.713785	27.794586
262.468639	12736.738150	27.799604
262.794850	12752.717343	27.804621
262.911738	12761.833502	27.809639
263.455680	12772.257882	27.814656
263.176858	12792.719843	27.819674
263.305074	12803.655890	27.824692
263.368794	12826.644090	27.829709
263.877189	12840.516171	27.834727
264.343755	12863.524411	27.839744
264.419770	12885.273572	27.844762
264.663480	12891.448652	27.849780
264.738444	12919.416571	27.854797
265.270516	12938.263122	27.859815
265.349843	12959.141929	27.864832
265.745827	12978.857322	27.869850
265.725035	12998.433710	27.874868
266.222382	13028.259244	27.879885
266.242361	13045.729811	27.884903
266.671264	13058.486876	27.889920
266.682284	13093.360352	27.894938
267.612568	13101.402800	27.899956
267.770781	13132.627357	27.904973
267.968813	13148.670708	27.909991
268.461367	13160.560009	27.915008
268.760049	13178.542464	27.920026
269.288784	13192.414631	27.925044
269.589704	13208.921671	27.930061
269.802203	13227.458993	27.935079
269.737555	13225.893792	27.940096
269.807887	13249.396827	27.945114
270.530968	13255.831520	27.950132
270.873496	13279.180798	27.955149
270.985817	13285.651993	27.960167
271.298504	13299.014738	27.965184
271.305867	13314.700556	27.970202
271.698722	13343.168161	27.975220
271.744211	13356.130766	27.980237
272.259898	13376.066370	27.985255
272.858552	13385.489238	27.990272
272.649876	13415.156562	27.995290
272.839397	13408.526687	28.000308
273.054460	13442.650072	28.005325
273.709908	13470.050054	28.010343
274.002394	13487.383002	28.015360
274.055894	13504.164541	28.020378
274.382530	13526.714638	28.025396
274.396452	13549.855513	28.030413
274.726106	13554.910286	28.035431
275.203098	13578.923284	28.040448
275.329229	13596.384748	28.045466
275.975224	13610.519963	28.050484
276.211623	13635.299396	28.055501
276.140046	13648.855269	28.060519
276.860621	13663.595969	28.065536
277.037149	13672.989595	28.070554
277.063328	13696.703884	28.075572
277.461913	13715.395348	28.080589
277.804501	13736.601927	28.085607
277.950701	13752.219479	28.090624
278.103898	13775.265123	28.095642
278.562532	13786.263757	28.100660
279.032122	13804.595275	28.105677
278.930722	13824.086707	28.110695
279.621717	13832.128159	28.115712
279.389373	13857.437835	28.120730
280.042091	13863.008164	28.125748
280.249174	13876.688305	28.130765
280.310337	13896.860540	28.135783
280.973844	13909.065661	28.140800
281.122981	13933.480174	28.145818
281.436760	13937.079886	28.150836
281.570063	13951.981104	28.155853
281.784525	13968.525289	28.160871
281.866916	13993.233047	28.165888
281.697503	14018.921831	28.170906
282.308632	14031.993069	28.175924
282.405939	14052.608678	28.180941
282.704177	14080.398207	28.185959
283.137724	14104.694974	28.190976
283.472333	14125.725290	28.195994
283.978232	14142.676881	28.201012
284.457438	14163.377559	28.206029
284.373268	14189.148637	28.211047
284.484059	14199.388745	28.216064
284.957803	14218.155026	28.221082
285.472201	14246.011497	28.226100
285.894508	14262.458533	28.231117
286.053679	14285.401464	28.236135
286.783056	14290.700780	28.241152
286.446192	14316.554864	28.246170
286.953980	14333.851496	28.251188
287.494564	14352.677790	28.256205
287.584932	14366.579396	28.261223
287.690814	14381.071041	28.266240
287.954099	14404.551675	28.271258
288.250202	14424.742408	28.276276
288.408216	14442.420145	28.281293
288.910407	14476.821250	28.286311
289.686968	14488.516362	28.291328
289.493588	14507.744869	28.296346
290.043721	14528.391716	28.301364
290.254443	14542.004041	28.306381
290.333324	14560.230868	28.311399
291.084159	14582.512042	28.316416
290.959672	14597.880483	28.321434
291.626244	14618.910068	28.326452
291.946184	14629.481475	28.331469
292.166961	14661.212395	28.336487
292.705923	14663.375436	28.341504
292.708964	14685.772655	28.346522
293.061959	14691.741200	28.351540
293.210935	14706.046326	28.356557
293.530422	14731.032742	28.361575
293.920095	14743.821265	28.366592
294.074083	14770.798941	28.371610
294.229856	14799.541591	28.376628
294.731603	14809.112145	28.381645
294.700451	14822.523599	28.386663
295.530629	14841.903012	28.391680
295.413148	14859.097234	28.396698
295.482190	14889.203537	28.401716
295.950537	14904.228259	28.406733
296.044912	14944.460085	28.411751
296.395675	14947.278457	28.416768
296.790741	14973.928133	28.421786
297.182384	15000.020476	28.426804
297.297381	15017.943948	28.431821
297.471029	15056.309416	28.436839
298.134826	15065.148772	28.441856
298.240916	15089.069350	28.446874
298.352160	15110.126871	28.451892
298.378720	15127.209266	28.456909
298.816521	15156.455922	28.461927
299.488172	15181.327989	28.466944
299.922162	15200.715093	28.471962
299.845086	15225.462135	28.476980
300.621217	15233.420844	28.481997
300.462772	15259.060888	28.487015
301.248786	15269.762033	28.492032
301.405325	15296.557318	28.497050
301.936314	15299.196185	28.502068
302.318327	15328.250637	28.507085
302.617300	15345.091147	28.512103
302.579417	15354.016864	28.517120
302.964768	15363.334339	28.522138
303.241065	15382.298558	28.527156
303.466173	15400.631357	28.532173
303.379813	15428.113285	28.537191
304.160014	15439.824242	28.542208
304.206634	15466.248688	28.547226
304.235544	15486.475500	28.552244
304.947498	15504.414171	28.557261
304.758332	15539.891827	28.562279
305.166303	15564.893236	28.567296
305.613577	15588.751759	28.572314
305.857184	15616.880777	28.577332
306.515276	15633.777200	28.582349
306.832714	15664.620857	28.587367
307.250956	15678.217112	28.592384
307.266816	15708.163488	28.597402
307.459317	15725.641452	28.602420
307.990281	15745.104565	28.607437
308.062039	15776.053722	28.612455
308.601897	15796.087580	28.617472
309.184673	15820.515081	28.622490
309.310304	15843.246648	28.627508
310.109654	15868.915088	28.632525
310.064869	15876.806669	28.637543
310.322717	15896.773845	28.642560
310.753598	15911.499911	28.647578
310.926526	15934.384547	28.652596
311.341099	15952.437559	28.657613
311.313328	15974.925169	28.662631
312.197727	16002.447543	28.667648
312.148293	16018.339218	28.672666
312.279320	16036.090914	28.677684
312.961773	16059.364246	28.682701
313.205927	16082.532050	28.687719
313.458379	16103.980436	28.692736
313.864240	16125.031468	28.697754
314.046685	16149.459523	28.702772
314.815796	16165.444400	28.707789
314.678836	16185.163608	28.712807
315.241838	16212.933410	28.717824
315.539931	16226.037733	28.722842
315.754177	16250.801139	28.727860
315.956177	16265.871198	28.732877
316.202631	16290.827938	28.737895
316.600245	16305.233583	28.742912
316.945824	16323.474961	28.747930
316.858456	16348.644668	28.752948
317.689149	16371.886025	28.757965
317.789223	16399.996002	28.762983
318.221740	16417.062976	28.768000
318.726066	16434.649277	28.773018
318.933434	16446.857721	28.778036
319.361708	16467.166220	28.783053
319.429280	16487.709413	28.788071
319.953910	16503.422990	28.793088
320.235383	16523.528876	28.798106
320.362058	16544.372880	28.803124
320.671762	16563.198948	28.808141
320.904721	16584.517203	28.813159
321.067637	16609.500862	28.818176
321.299314	16634.676516	28.823194
321.581715	16661.360184	28.828212
321.968775	16680.285496	28.833229
321.911051	16708.095828	28.838247
322.499760	16731.588968	28.843264
322.939144	16754.228872	28.848282
323.040177	16793.819405	28.853300
323.432350	16804.205290	28.858317
323.634679	16836.827748	28.863335
324.268934	16860.105462	28.868352
324.482931	16878.720746	28.873370
324.603433	16914.191072	28.878388
325.372269	16931.147739	28.883405
325.730120	16960.029367	28.888423
326.146925	16977.473105	28.893440
326.728541	16997.690670	28.898458
327.063581	17022.197215	28.903476
327.442228	17028.354678	28.908493
327.472188	17053.064669	28.913511
328.111708	17077.804633	28.918528
328.403706	17089.646451	28.923546
328.524980	17114.853720	28.928564
329.112727	17124.359378	28.933581
329.463227	17147.474817	28.938599
329.616247	17166.080025	28.943616
330.022608	17182.925131	28.948634
330.298716	17211.823882	28.953652
330.876544	17222.322746	28.958669
330.801174	17250.850983	28.963687
331.041102	17264.824857	28.968704
331.203185	17293.800948	28.973722
331.449773	17327.211516	28.978740
332.109498	17350.569252	28.983757
332.276801	17375.310584	28.988775
332.408667	17401.711400	28.993792
332.933076	17427.241772	28.998810
332.953820	17464.799526	29.003828
333.300123	17494.446949	29.008845
333.765313	17517.455644	29.013863
334.314761	17537.455353	29.018880
334.476232	17565.290739	29.023898
334.646082	17603.252895	29.028916
335.192544	17629.058943	29.033933
335.632157	17653.958967	29.038951
336.247433	17672.707344	29.043968
336.527452	17692.346710	29.048986
336.915145	17724.894518	29.054004
337.524656	17742.649238	29.059021
337.916315	17763.444608	29.064039
338.229329	17777.466719	29.069056
338.439508	17804.769511	29.074074
338.030620	17834.094849	29.079092
338.874254	17851.460977	29.084109
339.364303	17877.210541	29.089127
339.614969	17898.557507	29.094144
340.547222	17916.377222	29.099162
340.625267	17946.605828	29.104180
341.175829	17957.610968	29.109197
341.394408	17973.308818	29.114215
341.804620	17986.917767	29.119232
342.255536	18012.916784	29.124250
342.308148	18021.505795	29.129268
342.881430	18038.319414	29.134285
342.957025	18055.502333	29.139303
343.473756	18072.446730	29.144320
343.496936	18087.164978	29.149338
343.715548	18119.577600	29.154356
344.125681	18123.099237	29.159373
344.308680	18152.330317	29.164391
344.417344	18165.699265	29.169408
344.626263	18187.261598	29.174426
344.755204	18221.144290	29.179444
345.231927	18238.860042	29.184461
345.254221	18267.370701	29.189479
345.793960	18304.056233	29.194496
346.238308	18331.084665	29.199514
346.310258	18366.244534	29.204532
346.761692	18386.529484	29.209549
347.054370	18428.836761	29.214567
347.297753	18456.767278	29.219584
347.853197	18483.235273	29.224602
348.211700	18525.733685	29.229620
348.774081	18554.306778	29.234637
348.818706	18582.503718	29.239655
349.212168	18612.102765	29.244672
349.328730	18645.115010	29.249690
350.009175	18667.200548	29.254708
350.168237	18703.819122	29.259725
350.496391	18741.549575	29.264743
351.121525	18768.592935	29.269760
351.587693	18796.424086	29.274778
351.847384	18837.966965	29.279796
352.457099	18872.099308	29.284813
353.037017	18888.808643	29.289831
353.210824	18918.893887	29.294848
353.620218	18945.919643	29.299866
354.026153	18979.624026	29.304884
354.591348	18999.335969	29.309901
354.743687	19029.387130	29.314919
355.253927	19060.057000	29.319936
355.712368	19075.988922	29.324954
356.056204	19108.813121	29.329972
356.331430	19127.307280	29.334989
356.908260	19154.783342	29.340007
357.019948	19176.673618	29.345024
357.296292	19186.134266	29.350042
357.734305	19216.106949	29.355060
357.908351	19245.838026	29.360077
358.522483	19264.055530	29.365095
358.475720	19299.189714	29.370112
359.137294	19324.545798	29.375130
359.137320	19357.906655	29.380148
359.742225	19379.256792	29.385165
360.082030	19405.271643	29.390183
360.165648	19436.492082	29.395200
360.905392	19460.588397	29.400218
361.489794	19497.050021	29.405236
361.580968	19521.613224	29.410253
361.929522	19546.349848	29.415271
362.270377	19575.090633	29.420288
362.854412	19593.758065	29.425306
363.047202	19631.815629	29.430324
363.761449	19648.908668	29.435341
363.965716	19679.316584	29.440359
364.212530	19716.934999	29.445376
364.851023	19730.364124	29.450394
365.209589	19754.311119	29.455412
365.059463	19774.284266	29.460429
365.608321	19800.769631	29.465447
365.633813	19827.475672	29.470464
366.322705	19850.595611	29.475482
366.483720	19889.072079	29.480500
366.654828	19918.322404	29.485517
367.257304	19936.211490	29.490535
367.534517	19971.520485	29.495552
368.295097	19985.492449	29.500570
367.954545	20013.818613	29.505588
368.552831	20049.717879	29.510605
369.040935	20075.999319	29.515623
369.063890	20102.559593	29.520640
369.476879	20131.224752	29.525658
369.885205	20165.680010	29.530676
370.334521	20191.351600	29.535693
370.813929	20219.482484	29.540711
371.138436	20255.623003	29.545728
371.512437	20273.764686	29.550746
372.053039	20305.128675	29.555764
372.365556	20332.139595	29.560781
372.583605	20357.168618	29.565799
373.232968	20393.291928	29.570816
373.515012	20415.551356	29.575834
373.736058	20444.023361	29.580852
374.107096	20485.182961	29.585869
374.469450	20514.278115	29.590887
374.524926	20544.248693	29.595904
375.154277	20584.523858	29.600922
375.418623	20616.681480	29.605940
375.681297	20647.540284	29.610957
376.313289	20683.501545	29.615975
376.617601	20718.487564	29.620992
377.290944	20754.063735	29.626010
377.711381	20788.081531	29.631028
378.274445	20828.231082	29.636045
378.786448	20841.656811	29.641063
378.588429	20873.990781	29.646080
379.079375	20903.517829	29.651098
379.532002	20939.537704	29.656116
380.037415	20966.626507	29.661133
380.886282	20981.186985	29.666151
380.913677	21024.812367	29.671168
381.464563	21041.921257	29.676186
381.592117	21078.755195	29.681204
381.661797	21108.443774	29.686221
382.516901	21131.288855	29.691239
382.647679	21168.667990	29.696256
383.246964	21191.164473	29.701274
383.566736	21230.207414	29.706292
384.028651	21261.434848	29.711309
384.495349	21281.746011	29.716327
384.680261	21319.488623	29.721344
385.182124	21338.091189	29.726362
385.542612	21369.732941	29.731380
385.491610	21398.831816	29.736397
386.600120	21424.768292	29.741415
386.845413	21461.075873	29.746432
387.180310	21486.793606	29.751450
387.470573	21513.562558	29.756468
387.898303	21544.553358	29.761485
388.096979	21570.230695	29.766503
388.257522	21605.628648	29.771520
388.995443	21635.239086	29.776538
389.697988	21669.598271	29.781556
390.054809	21689.250112	29.786573
390.747828	21707.075648	29.791591
390.739385	21739.225374	29.796608
390.950113	21766.444650	29.801626
391.416558	21794.514089	29.806644
391.748184	21827.597899	29.811661
392.724343	21835.870448	29.816679
393.091341	21878.112617	29.821696
393.283970	21898.911379	29.826714
393.498751	21912.652055	29.831732
393.723887	21941.516947	29.836749
394.086778	21961.724700	29.841767
394.231108	21997.906657	29.846784
395.024918	22011.056473	29.851802
394.942795	22039.564002	29.856820
395.172940	22078.089208	29.861837
395.513305	22096.665730	29.866855
395.549998	22142.337539	29.871872
396.204873	22172.009969	29.876890
396.500358	22202.227584	29.881908
396.842732	22248.580717	29.886925
397.333198	22289.299214	29.891943
397.683638	22331.419110	29.896960
398.143254	22366.193620	29.901978
398.750794	22410.757785	29.906996
398.794201	22440.350555	29.912013
399.502630	22473.206119	29.917031
400.036386	22517.005405	29.922048
400.226628	22550.216519	29.927066
400.844164	22588.908985	29.932084
401.253881	22628.567842	29.937101
401.900623	22655.429400	29.942119
402.060548	22681.406548	29.947136
402.509442	22719.352997	29.952154
403.197871	22754.274923	29.957172
403.476212	22795.958504	29.962189
404.211234	22811.706282	29.967207
404.455932	22843.690053	29.972224
404.471023	22876.112407	29.977242
404.827239	22909.025533	29.982260
405.300413	22951.391566	29.987277
405.814317	22977.556571	29.992295
406.025317	23031.541951	29.997312
406.477396	23054.938866	30.002330
406.920079	23094.810963	30.007348
407.236262	23140.166395	30.012365
408.110416	23172.516517	30.017383
408.059573	23215.578611	30.022400
408.740346	23236.747633	30.027418
409.276474	23274.605194	30.032436
409.430716	23312.399891	30.037453
410.227716	23346.697963	30.042471
410.654207	23379.343334	30.047488
410.944689	23422.612802	30.052506
411.525670	23443.940521	30.057524
411.380268	23480.969923	30.062541
412.087085	23515.874604	30.067559
412.389403	23556.225163	30.072576
412.784551	23595.330457	30.077594
413.373612	23629.496361	30.082612
413.617361	23667.412646	30.087629
414.301609	23699.481393	30.092647
414.723619	23731.746564	30.097664
414.983728	23763.081392	30.102682
415.163526	23795.858275	30.107700
415.578404	23840.051223	30.112717
416.613149	23863.092622	30.117735
417.006410	23896.767922	30.122752
417.121877	23927.534058	30.127770
417.632353	23953.522937	30.132788
418.086718	23997.299749	30.137805
418.781630	24026.014736	30.142823
419.011563	24063.000626	30.147840
419.320145	24095.479224	30.152858
419.860457	24117.631388	30.157876
420.224466	24154.440743	30.162893
420.814901	24187.046335	30.167911
421.281399	24217.404808	30.172928
421.323672	24241.065146	30.177946
422.138048	24268.767273	30.182964
422.138353	24300.761108	30.187981
422.524340	24324.080818	30.192999
423.021535	24353.929817	30.198016
422.957314	24381.007965	30.203034
423.705879	24401.441803	30.208052
423.530206	24451.266166	30.213069
423.741388	24486.811544	30.218087
424.569289	24527.257190	30.223104
424.669993	24573.374359	30.228122
425.345741	24615.359326	30.233140
425.651007	24662.143072	30.238157
426.111493	24706.743891	30.243175
426.495194	24745.519382	30.248192
426.893328	24795.486332	30.253210
427.680406	24839.361630	30.258228
428.090103	24878.839632	30.263245
428.820050	24910.751697	30.268263
428.793213	24943.467198	30.273280
429.287628	24988.097828	30.278298
429.802804	25017.724223	30.283316
430.459860	25065.065897	30.288333
430.888440	25098.302449	30.293351
431.517170	25136.826947	30.298368
431.667248	25173.941998	30.303386
432.289393	25221.170024	30.308404
432.764897	25261.732503	30.313421
433.001950	25290.358220	30.318439
433.607094	25330.136100	30.323456
433.905541	25377.216261	30.328474
434.516376	25404.225303	30.333492
435.279034	25441.558123	30.338509
435.525451	25475.327067	30.343527
435.815763	25507.748281	30.348544
436.076901	25550.996441	30.353562
437.186597	25579.178570	30.358580
437.398381	25624.860668	30.363597
437.744954	25654.452981	30.368615
438.036852	25690.706654	30.373632
438.470222	25732.529444	30.378650
438.975422	25762.622448	30.383668
439.219105	25807.571121	30.388685
439.902304	25841.555534	30.393703
440.287491	25876.374745	30.398720
440.423064	25915.995124	30.403738
441.225056	25954.625261	30.408756
441.501978	25995.692322	30.413773
441.833920	26038.523086	30.418791
442.546311	26075.729969	30.423808
442.633691	26117.301832	30.428826
443.598570	26150.476897	30.433844
443.532735	26192.768247	30.438861
443.913723	26221.346457	30.443879
444.525036	26267.014604	30.448896
444.866496	26316.515892	30.453914
445.300090	26358.986805	30.458932
445.823141	26406.307034	30.463949
446.240758	26447.594771	30.468967
446.503243	26482.280948	30.473984
446.905581	26533.624399	30.479002
447.705913	26566.354342	30.484020
448.381270	26609.400965	30.489037
448.655868	26651.933609	30.494055
449.323250	26693.814635	30.499072
449.415248	26733.027717	30.504090
450.231780	26759.279331	30.509108
450.462339	26800.182484	30.514125
450.709612	26831.096028	30.519143
451.253263	26867.676424	30.524160
451.446939	26908.084380	30.529178
452.166207	26938.929468	30.534196
452.557049	26976.409166	30.539213
452.948061	27017.623806	30.544231
453.702936	27046.441180	30.549248
453.798610	27090.950824	30.554266
454.353247	27125.757129	30.559284
454.771663	27164.431376	30.564301
455.187973	27211.408707	30.569319
455.581065	27238.781577	30.574336
455.770105	27289.257225	30.579354
456.670488	27329.069721	30.584372
456.936746	27371.324759	30.589389
457.067687	27415.592809	30.594407
457.700509	27455.263757	30.599424
458.409018	27503.732942	30.604442
458.758545	27549.365781	30.609460
459.138483	27595.564684	30.614477
459.445291	27639.640162	30.619495
460.224545	27680.123355	30.624512
460.503583	27725.705231	30.629530
461.377181	27769.084711	30.634548
461.672156	27817.837723	30.639565
461.867816	27859.253886	30.644583
462.827781	27895.578279	30.649600
463.272222	27935.587499	30.654618
463.711941	27973.329407	30.659636
464.136248	28012.061351	30.664653
464.418768	28061.325005	30.669671
465.365640	28093.390039	30.674688
465.466750	28145.012092	30.679706
465.947448	28175.463521	30.684724
466.511913	28225.794582	30.689741
466.699228	28272.516138	30.694759
467.324455	28314.808704	30.699776
467.539412	28369.488416	30.704794
468.094240	28404.079580	30.709812
468.759681	28467.717011	30.714829
469.240470	28504.913816	30.719847
469.770261	28544.383471	30.724864
470.148837	28587.256978	30.729882
470.898103	28631.085079	30.734900
471.269930	28676.840219	30.739917
471.760404	28719.342199	30.744935
472.025304	28755.389071	30.749952
472.161420	28802.221470	30.754970
472.752172	28850.297464	30.759988
473.397296	28900.339503	30.765005
473.741025	28955.450877	30.770023
474.658947	28994.245285	30.775040
474.679154	29030.279585	30.780058
475.351390	29083.983578	30.785076
475.568296	29114.003920	30.790093
476.282665	29169.691913	30.795111
477.276120	29211.957267	30.800128
477.433152	29255.541064	30.805146
478.153140	29298.094808	30.810164
478.643248	29340.386984	30.815181
478.579844	29380.900008	30.820199
479.290659	29418.669589	30.825216
479.550877	29471.575358	30.830234
480.089435	29516.346011	30.835252
480.551810	29556.415926	30.840269
481.156314	29613.896583	30.845287
481.470840	29649.861366	30.850304
481.831406	29702.173871	30.855322
482.365351	29734.934946	30.860340
482.985846	29769.795585	30.865357
483.097858	29823.452584	30.870375
483.787986	29854.257193	30.875392
484.054618	29910.078425	30.880410
484.576013	29955.155919	30.885428
485.072182	29994.684893	30.890445
485.343797	30040.403392	30.895463
485.959410	30082.200182	30.900480
486.282062	30152.036985	30.905498
486.918885	30197.168565	30.910516
487.740691	30240.802550	30.915533
487.939822	30300.018405	30.920551
488.295215	30330.639460	30.925568
488.667133	30386.706653	30.930586
489.335244	30439.882277	30.935604
489.799552	30492.722643	30.940621
489.921215	30549.339738	30.945639
490.891427	30597.556504	30.950656
491.440773	30657.513850	30.955674
491.881604	30713.343510	30.960692
492.445089	30761.949858	30.965709
492.883012	30813.561893	30.970727
493.761190	30857.945320	30.975744
494.011139	30905.360816	30.980762
494.752144	30950.376124	30.985780
495.337308	30995.707613	30.990797
495.594846	31050.959724	30.995815
496.599255	31091.830053	31.000832
496.959474	31138.814598	31.005850
497.095116	31185.445184	31.010868
497.873596	31230.420299	31.015885
498.462001	31274.691813	31.020903
499.102452	31320.633415	31.025920
499.268506	31371.676800	31.030938
499.762972	31416.734097	31.035956
500.298959	31457.039117	31.040973
500.795254	31512.590776	31.045991
501.440464	31555.010912	31.051008
501.592213	31600.251602	31.056026
501.999156	31656.664118	31.061044
502.697618	31704.525008	31.066061
503.266920	31755.720488	31.071079
503.567986	31801.763677	31.076096
504.245498	31861.565069	31.081114
504.910258	31908.097380	31.086132
505.531640	31956.609088	31.091149
505.816167	32006.628141	31.096167
506.115764	32049.630446	31.101184
506.701984	32105.251125	31.106202
507.295047	32166.323363	31.111220
507.766148	32209.433358	31.116237
508.120674	32254.219338	31.121255
508.823830	32308.909392	31.126272
509.130543	32359.834529	31.131290
509.418222	32413.236824	31.136308
510.203870	32469.813296	31.141325
510.653976	32522.857721	31.146343
511.357421	32569.937573	31.151360
511.952981	32629.332286	31.156378
512.250642	32680.559610	31.161396
513.066015	32731.426884	31.166413
513.453570	32785.785663	31.171431
513.816420	32826.608398	31.176448
514.636966	32880.832707	31.181466
514.232866	32927.670788	31.186484
515.145901	32973.587349	31.191501
515.320686	33046.104384	31.196519
516.130445	33089.842074	31.201536
516.741643	33146.023569	31.206554
516.988455	33205.443204	31.211572
517.817148	33251.346040	31.216589
518.264902	33300.158376	31.221607
519.111844	33346.863116	31.226624
519.295496	33397.325624	31.231642
519.581294	33446.417610	31.236660
520.652421	33491.094435	31.241677
520.810653	33553.707605	31.246695
521.161215	33596.238182	31.251712
522.089615	33653.129296	31.256730
522.209362	33707.106033	31.261748
523.036002	33763.190709	31.266765
523.205176	33819.936601	31.271783
523.953210	33871.771295	31.276800
524.280930	33915.843237	31.281818
524.722552	33973.017887	31.286836
525.853715	34034.165278	31.291853
526.130678	34090.591243	31.296871
526.799611	34133.660539	31.301888
527.023954	34189.439129	31.306906
527.625131	34241.693667	31.311924
528.412453	34294.116368	31.316941
528.701896	34352.573409	31.321959
529.516611	34403.928402	31.326976
530.227265	34468.179576	31.331994
530.627519	34514.711982	31.337012
531.361220	34562.748304	31.342029
531.850426	34629.356225	31.347047
532.274337	34672.170716	31.352064
532.751781	34719.050644	31.357082
533.051374	34775.086850	31.362100
533.769924	34829.955664	31.367117
534.295590	34883.360680	31.372135
534.884459	34937.048894	31.377152
535.611022	34985.702928	31.382170
535.717880	35048.200430	31.387188
536.449474	35102.821760	31.392205
536.930479	35165.260913	31.397223
537.376087	35219.169343	31.402240
538.197632	35271.270491	31.407258
538.223292	35331.510135	31.412276
539.286515	35386.437231	31.417293
539.816289	35447.550102	31.422311
540.273394	35493.160404	31.427328
540.855457	35556.874989	31.432346
541.328086	35615.886530	31.437364
542.083104	35661.425869	31.442381
542.450818	35718.154375	31.447399
542.997196	35774.743035	31.452416
543.451623	35820.910071	31.457434
544.187716	35893.380455	31.462452
545.028076	35942.119242	31.467469
545.337422	35991.567774	31.472487
545.624456	36045.896270	31.477504
546.414220	36101.309494	31.482522
546.854132	36167.407355	31.487540
547.666824	36220.052409	31.492557
548.035386	36278.395306	31.497575
548.558778	36323.333955	31.502592
549.209536	36381.141290	31.507610
549.435711	36437.715577	31.512628
550.415789	36482.408623	31.517645
550.757708	36543.890844	31.522663
551.160247	36589.121582	31.527680
551.795921	36641.831875	31.532698
552.014321	36700.283041	31.537716
553.012924	36743.622818	31.542733
553.326169	36796.617317	31.547751
553.605631	36838.151031	31.552768
554.528780	36899.775001	31.557786
554.639296	36961.871365	31.562804
555.514472	37000.936547	31.567821
555.430520	37063.286372	31.572839
556.133346	37118.164756	31.577856
556.775505	37180.738868	31.582874
557.124128	37243.115578	31.587892
557.869329	37303.804544	31.592909
558.292756	37355.772430	31.597927
558.891818	37424.364118	31.602944
559.310556	37490.154677	31.607962
559.809171	37553.514501	31.612980
560.580776	37618.969380	31.617997
561.139027	37690.112842	31.623015
561.595378	37754.544054	31.628032
562.345930	37814.990803	31.633050
562.642783	37884.221318	31.638068
563.642957	37941.745395	31.643085
563.835085	38009.024116	31.648103
564.404324	38076.483731	31.653120
565.084763	38134.496910	31.658138
566.044686	38208.116866	31.663156
566.685105	38264.760869	31.668173
567.283537	38342.509862	31.673191
567.935570	38400.904210	31.678208
568.678058	38460.028711	31.683226
569.009869	38519.789528	31.688244
569.668707	38570.282561	31.693261
570.557731	38636.125702	31.698279
570.647447	38692.196128	31.703296
571.527221	38747.766683	31.708314
572.039267	38813.215140	31.713332
572.542292	38868.359135	31.718349
572.981938	38934.337681	31.723367
573.811381	38995.378197	31.728384
574.429027	39060.200843	31.733402
574.644557	39125.453265	31.738420
575.629521	39179.925013	31.743437
576.190463	39240.202678	31.748455
576.586757	39291.160977	31.753472
577.356459	39352.275701	31.758490
577.408000	39425.274332	31.763508
578.249798	39485.054929	31.768525
578.750444	39540.475971	31.773543
579.179240	39617.008403	31.778560
579.762764	39673.621991	31.783578
580.451074	39744.748776	31.788596
581.142440	39797.023358	31.793613
581.741464	39862.132869	31.798631
582.156904	39925.666204	31.803648
583.097310	39983.781132	31.808666
583.179497	40053.992928	31.813684
584.052528	40121.166742	31.818701
584.385152	40184.544207	31.823719
584.713858	40259.454342	31.828736
585.926587	40323.160181	31.833754
586.228466	40387.569397	31.838772
586.902331	40460.964787	31.843789
587.699056	40528.209536	31.848807
588.049419	40578.790711	31.853824
588.728505	40639.972067	31.858842
589.024201	40706.564816	31.863860
589.649888	40773.046381	31.868877
590.318453	40851.457348	31.873895
591.149475	40907.528677	31.878912
592.066660	40958.067617	31.883930
592.527354	41025.335053	31.888948
592.987492	41080.978951	31.893965
593.452887	41130.257727	31.898983
593.631803	41192.521270	31.904000
594.709429	41251.454091	31.909018
595.154187	41315.063128	31.914036
595.674017	41372.677457	31.919053
596.350261	41435.178385	31.924071
596.826789	41504.212865	31.929088
597.252080	41561.357242	31.934106
598.035186	41630.934990	31.939124
598.702948	41691.594476	31.944141
599.212075	41755.052307	31.949159
599.658499	41815.679367	31.954176
600.190195	41883.474874	31.959194
600.669774	41953.981724	31.964212
601.167211	42022.051759	31.969229
602.297858	42089.136439	31.974247
602.591680	42156.214593	31.979264
603.060190	42226.556981	31.984282
603.599729	42299.593562	31.989300
604.451731	42371.947299	31.994317
605.137771	42439.807700	31.999335
605.930578	42508.976703	32.004352
606.450968	42568.517380	32.009370
606.924568	42646.993459	32.014388
607.391393	42723.908164	32.019405
608.464953	42788.984194	32.024423
608.951548	42869.366030	32.029440
609.835757	42919.025434	32.034458
610.269085	42994.106115	32.039476
610.927341	43062.216492	32.044493
611.426068	43129.504201	32.049511
612.038418	43212.496733	32.054528
612.614645	43277.161059	32.059546
613.728009	43343.217524	32.064564
614.284948	43408.175970	32.069581
614.830667	43469.192967	32.074599
615.145533	43545.994121	32.079616
615.981252	43598.189248	32.084634
616.818912	43670.951388	32.089652
617.190687	43740.197777	32.094669
618.041430	43807.537036	32.099687
618.728344	43877.205402	32.104704
619.564952	43936.874940	32.109722
620.060144	44004.605266	32.114740
620.289001	44063.845313	32.119757
620.969607	44130.295065	32.124775
621.263284	44209.963106	32.129792
622.094500	44272.226891	32.134810
622.704566	44346.756458	32.139828
623.405739	44417.074916	32.144845
624.093697	44476.243462	32.149863
624.142180	44560.156214	32.154880
625.019456	44622.369335	32.159898
625.625936	44699.951084	32.164916
626.343856	44772.099483	32.169933
627.154894	44844.671656	32.174951
627.833081	44918.191264	32.179968
628.474360	44984.476878	32.184986
629.094903	45056.121473	32.190004
629.959818	45115.199601	32.195021
630.461581	45177.824029	32.200039
630.794450	45260.341378	32.205056
631.571500	45326.242602	32.210074
632.393221	45397.381560	32.215092
632.539394	45461.366724	32.220109
633.153063	45523.784324	32.225127
633.453710	45588.773770	32.230144
634.188018	45660.613405	32.235162
634.458795	45740.961144	32.240180
635.314481	45810.071933	32.245197
636.220255	45878.612607	32.250215
636.554157	45956.067787	32.255232
637.075557	46025.591499	32.260250
637.811208	46109.653225	32.265268
638.174649	46179.936245	32.270285
639.167658	46253.048976	32.275303
639.331171	46335.387461	32.280320
640.490295	46414.113215	32.285338
640.823339	46490.645473	32.290356
641.362850	46573.686984	32.295373
642.455114	46652.036372	32.300391
642.885001	46729.920935	32.305408
643.752362	46814.355573	32.310426
644.355562	46891.264751	32.315444
645.127330	46976.947517	32.320461
646.030016	47042.739194	32.325479
646.358675	47129.452817	32.330496
647.534623	47195.720878	32.335514
648.048572	47278.671801	32.340532
648.201680	47341.452647	32.345549
649.224589	47424.051568	32.350567
649.988998	47503.330321	32.355584
650.428365	47568.483600	32.360602
651.316045	47641.546470	32.365620
652.035079	47725.624411	32.370637
652.918783	47803.766723	32.375655
653.158143	47878.999986	32.380672
654.032952	47952.397776	32.385690
654.757973	48031.262053	32.390708
654.918229	48103.054312	32.395725
655.857924	48174.588403	32.400743
656.442460	48261.460639	32.405760
656.908558	48346.432701	32.410778
657.576959	48430.825305	32.415796
657.931017	48503.885013	32.420813
658.934493	48589.479840	32.425831
659.127743	48681.497106	32.430848
660.260631	48761.658107	32.435866
661.122141	48845.831096	32.440884
661.561976	48934.795816	32.445901
662.584155	49014.158200	32.450919
663.090628	49084.526163	32.455936
663.823084	49161.148322	32.460954
664.810139	49237.134904	32.465972
665.194728	49314.342664	32.470989
665.798418	49390.001643	32.476007
666.098883	49469.766403	32.481024
667.163713	49544.686446	32.486042
667.933183	49634.348397	32.491060
669.032970	49721.416773	32.496077
669.634997	49795.621605	32.501095
670.190795	49867.421343	32.506112
670.557828	49936.703729	32.511130
671.330142	50005.928789	32.516148
672.142364	50088.425609	32.521165
672.687883	50165.578570	32.526183
673.180476	50252.550817	32.531200
673.982821	50322.517445	32.536218
674.716316	50410.600237	32.541236
675.379351	50487.248631	32.546253
676.050364	50561.091238	32.551271
676.350903	50647.654840	32.556288
677.461822	50714.748104	32.561306
677.929776	50793.653605	32.566324
678.389653	50856.647862	32.571341
679.204643	50929.728949	32.576359
679.856414	51010.999133	32.581376
680.460240	51089.100026	32.586394
681.268562	51163.345466	32.591412
681.442402	51240.039867	32.596429
682.370077	51310.677915	32.601447
683.084899	51394.965260	32.606464
683.415876	51470.143684	32.611482
684.325992	51564.526165	32.616500
684.698388	51653.249223	32.621517
685.632558	51728.632090	32.626535
686.046486	51820.014993	32.631552
687.152638	51903.715454	32.636570
687.700119	51975.739173	32.641588
688.400728	52062.565084	32.646605
689.197264	52152.332133	32.651623
690.040622	52238.345515	32.656640
690.501841	52318.237543	32.661658
691.159864	52404.345494	32.666676
691.942770	52497.831166	32.671693
692.865285	52567.425896	32.676711
693.421216	52653.071687	32.681728
694.337819	52740.275532	32.686746
695.232488	52816.092430	32.691764
695.597192	52911.715181	32.696781
696.189190	52989.920416	32.701799
696.653558	53075.469482	32.706816
697.322548	53172.035068	32.711834
698.404948	53260.332069	32.716852
699.245423	53347.911337	32.721869
700.051226	53420.845337	32.726887
700.356980	53513.985176	32.731904
701.135247	53604.652750	32.736922
702.103950	53694.253076	32.741940
702.471383	53782.089442	32.746957
703.270344	53874.214316	32.751975
703.831576	53959.087804	32.756992
704.426156	54053.427090	32.762010
705.462662	54138.709226	32.767028
705.944753	54229.605588	32.772045
706.935934	54311.749490	32.777063
707.711577	54409.004835	32.782080
708.236500	54505.404935	32.787098
709.331800	54591.071040	32.792116
709.768379	54682.634126	32.797133
710.716617	54764.129906	32.802151
711.254203	54859.916755	32.807168
711.894543	54941.761170	32.812186
712.640601	55034.127679	32.817204
712.972393	55127.694167	32.822221
713.939032	55232.213544	32.827239
714.687757	55316.556364	32.832256
715.126078	55399.105860	32.837274
716.312619	55498.427960	32.842292
716.881103	55586.946777	32.847309
717.577174	55671.577840	32.852327
718.312387	55766.502310	32.857344
718.986389	55858.183200	32.862362
720.158077	55942.616681	32.867380
720.459198	56037.405736	32.872397
721.662753	56120.931113	32.877415
722.403378	56204.805135	32.882432
722.506722	56302.004061	32.887450
723.435995	56387.876012	32.892468
724.090753	56486.191531	32.897485
724.787005	56569.638422	32.902503
725.052354	56650.168055	32.907520
725.915020	56749.948085	32.912538
726.669677	56830.353266	32.917556
727.423837	56920.635592	32.922573
727.973890	56995.388102	32.927591
728.687971	57095.049097	32.932608
729.403568	57195.298021	32.937626
730.273402	57271.294095	32.942644
730.681066	57366.286686	32.947661
731.582551	57467.618408	32.952679
732.154249	57558.559404	32.957696
732.481168	57657.181367	32.962714
733.695868	57753.723229	32.967732
734.092476	57862.761611	32.972749
734.898127	57961.166846	32.977767
735.709006	58061.416977	32.982784
736.237224	58174.100558	32.987802
737.203364	58269.523234	32.992820
738.118790	58376.032921	32.997837
738.579132	58469.328374	33.002855
739.234336	58572.191512	33.007872
740.229882	58685.811786	33.012890
741.082068	58782.721904	33.017908
741.886917	58888.639585	33.022925
742.472175	58986.138331	33.027943
743.241711	59096.448844	33.032960
743.773143	59195.663845	33.037978
744.836636	59312.467910	33.042996
745.561003	59419.229585	33.048013
746.194709	59519.990267	33.053031
747.130638	59628.481302	33.058048
747.707693	59732.519823	33.063066
748.672232	59838.321260	33.068084
749.611828	59936.480130	33.073101
750.316472	60042.597388	33.078119
751.698275	60135.476333	33.083136
752.123598	60242.531975	33.088154
752.989705	60338.935311	33.093172
753.917395	60432.611235	33.098189
754.545127	60525.995918	33.103207
755.626323	60621.853078	33.108224
756.037210	60728.717738	33.113242
756.790981	60818.695242	33.118260
757.612008	60909.831281	33.123277
758.285686	61011.237420	33.128295
759.390164	61104.823989	33.133312
760.116822	61204.383088	33.138330
760.985081	61299.355876	33.143348
761.737482	61394.487322	33.148365
762.104404	61483.817535	33.153383
762.875415	61583.567080	33.158400
763.826052	61681.454431	33.163418
764.744949	61772.868878	33.168436
765.243732	61867.102704	33.173453
765.911329	61969.134021	33.178471
767.216840	62058.431574	33.183488
767.716904	62170.421417	33.188506
768.490052	62257.854796	33.193524
769.115949	62360.836751	33.198541
769.706572	62459.653317	33.203559
770.553671	62548.042784	33.208576
771.215091	62660.109737	33.213594
771.780978	62761.529726	33.218612
772.605144	62870.119685	33.223629
773.469296	62975.587361	33.228647
774.278954	63070.483227	33.233664
774.842304	63178.808226	33.238682
775.578201	63277.446658	33.243700
776.509196	63372.406017	33.248717
777.107882	63472.016239	33.253735
777.882540	63564.758343	33.258752
778.360801	63664.547441	33.263770
779.357894	63759.573500	33.268788
780.070506	63865.519594	33.273805
780.544273	63967.327373	33.278823
781.399474	64064.179865	33.283840
782.232740	64175.227844	33.288858
783.035037	64268.866159	33.293876
784.062973	64379.465820	33.298893
784.944861	64481.689041	33.303911
785.814702	64580.564382	33.308928
786.507743	64680.038372	33.313946
787.673528	64786.040635	33.318964
787.948930	64881.937153	33.323981
788.524273	64994.738995	33.328999
789.417702	65095.680042	33.334016
790.418317	65214.930322	33.339034
791.071759	65322.417150	33.344052
791.805516	65429.701593	33.349069
792.586480	65532.692631	33.354087
793.690282	65644.007140	33.359104
794.441310	65763.719078	33.364122
795.270355	65854.862980	33.369140
796.010759	65966.195062	33.374157
796.498726	66083.543703	33.379175
797.418239	66178.170070	33.384192
798.400334	66310.516098	33.389210
799.425642	66417.574043	33.394228
799.918335	66536.264703	33.399245
800.678079	66641.698694	33.404263
801.841230	66753.458150	33.409280
802.381140	66871.371593	33.414298
803.520755	66975.113306	33.419316
804.287944	67080.820121	33.424333
805.094235	67193.077174	33.429351
805.804949	67305.129354	33.434368
806.734777	67413.504230	33.439386
807.872584	67522.275181	33.444404
808.650353	67635.196829	33.449421
809.212547	67742.116829	33.454439
810.456274	67844.264995	33.459456
811.103994	67954.314178	33.464474
811.737431	68062.317801	33.469492
812.751125	68168.861796	33.474509
813.283262	68277.003397	33.479527
814.324914	68380.742932	33.484544
814.675108	68497.710501	33.489562
815.581325	68603.844519	33.494580
816.497661	68712.424281	33.499597
817.276168	68829.740130	33.504615
818.249375	68936.693010	33.509632
819.104009	69048.496663	33.514650
819.929109	69170.959774	33.519668
820.678091	69276.686882	33.524685
821.459192	69392.987423	33.529703
822.433841	69499.076650	33.534720
822.707663	69617.327587	33.539738
823.762177	69732.415003	33.544756
824.769442	69840.979155	33.549773
825.398261	69950.466391	33.554791
826.274208	70059.337910	33.559808
826.866059	70180.662970	33.564826
827.814682	70304.465299	33.569844
828.940415	70416.882562	33.574861
829.529634	70527.802020	33.579879
830.619932	70627.807406	33.584896
831.050505	70746.329514	33.589914
831.939456	70844.674567	33.594932
832.788610	70959.619167	33.599949
833.488940	71067.595314	33.604967
834.639693	71169.224658	33.609984
835.090983	71279.430966	33.615002
836.147955	71389.645156	33.620020
837.273228	71491.805088	33.625037
837.481505	71603.747951	33.630055
838.435986	71714.455020	33.635072
839.409922	71833.158824	33.640090
840.210746	71943.424533	33.645108
840.920238	72051.182759	33.650125
841.853083	72172.449992	33.655143
842.753259	72284.465325	33.660160
843.199018	72403.891995	33.665178
844.104557	72516.919449	33.670196
845.043950	72634.381242	33.675213
845.606551	72767.159225	33.680231
846.965106	72879.904953	33.685248
847.469599	73008.672003	33.690266
848.225827	73127.810989	33.695284
849.130625	73252.895945	33.700301
849.948868	73395.450388	33.705319
851.055277	73501.050563	33.710336
851.959996	73630.925054	33.715354
852.634144	73757.094535	33.720372
853.747362	73887.473622	33.725389
854.491696	74012.032938	33.730407
855.797223	74139.915263	33.735424
856.179770	74249.983575	33.740442
857.106767	74375.292638	33.745460
858.171904	74503.634255	33.750477
858.783893	74632.437363	33.755495
859.961289	74757.719846	33.760512
860.827673	74882.991238	33.765530
861.612177	75009.832725	33.770548
862.909815	75132.466447	33.775565
863.275252	75258.720923	33.780583
864.214430	75373.648649	33.785600
865.304629	75506.368633	33.790618
865.971412	75643.953589	33.795636
866.906376	75747.518429	33.800653
867.645885	75877.250113	33.805671
868.869862	76004.119505	33.810688
869.632746	76129.035605	33.815706
870.830484	76260.135817	33.820724
872.014779	76376.868769	33.825741
872.561136	76497.591378	33.830759
873.644952	76619.256727	33.835776
874.096920	76737.276499	33.840794
875.049921	76866.915416	33.845812
876.242332	76971.721068	33.850829
876.578005	77112.861362	33.855847
877.325425	77224.756390	33.860864
878.305967	77349.852091	33.865882
879.086333	77481.825520	33.870900
880.175192	77609.694199	33.875917
880.830745	77748.546459	33.880935
881.953876	77874.152844	33.885952
882.677237	77986.669233	33.890970
883.444322	78121.185118	33.895988
884.518312	78249.850599	33.901005
884.895298	78387.045016	33.906023
885.933910	78515.838059	33.911040
886.959318	78642.869190	33.916058
887.942443	78775.038106	33.921076
888.685723	78898.739467	33.926093
889.284770	79016.443312	33.931111
890.377396	79135.033975	33.936128
891.332568	79263.465561	33.941146
892.075489	79377.326744	33.946164
893.134503	79511.480056	33.951181
893.791952	79631.214368	33.956199
894.800157	79757.324733	33.961216
895.722045	79881.134790	33.966234
896.265799	80020.677470	33.971252
897.325603	80138.785413	33.976269
898.338336	80267.681314	33.981287
898.987291	80395.676550	33.986304
899.998671	80532.405855	33.991322
901.134974	80666.142036	33.996340
901.705650	80789.433136	34.001357
902.667619	80938.749504	34.006375
903.524896	81065.708193	34.011392
904.288661	81196.453525	34.016410
905.226904	81342.663931	34.021428
906.113637	81474.668441	34.026445
906.967076	81634.382563	34.031463
907.889232	81762.226424	34.036480
908.695378	81903.274581	34.041498
909.671647	82052.298528	34.046516
910.590852	82192.969160	34.051533
911.230429	82337.982666	34.056551
912.499034	82475.940076	34.061568
913.852493	82617.015990	34.066586
914.511418	82765.413773	34.071604
915.380986	82905.091029	34.076621
915.996762	83057.686149	34.081639
917.567033	83196.281289	34.086656
918.287990	83342.502425	34.091674
918.977125	83493.854558	34.096692
920.184721	83627.918926	34.101709
921.073730	83780.321791	34.106727
921.851497	83921.709695	34.111744
922.935591	84071.690594	34.116762
923.774234	84217.132221	34.121780
925.042226	84366.913786	34.126797
925.794790	84512.080448	34.131815
926.800599	84656.408903	34.136832
927.616887	84804.357166	34.141850
928.403804	84945.553648	34.146868
929.435948	85093.581943	34.151885
930.272473	85243.731571	34.156903
931.469936	85390.082957	34.161920
932.025595	85539.838017	34.166938
933.446715	85696.411184	34.171956
934.729652	85827.198128	34.176973
935.516744	85978.600855	34.181991
936.360239	86122.250202	34.187008
937.171339	86269.170868	34.192026
938.179003	86416.414299	34.197044
939.104512	86548.447662	34.202061
940.191416	86701.893631	34.207079
940.931411	86846.520021	34.212096
942.201025	86991.983583	34.217114
942.922237	87134.324156	34.222132
944.139116	87278.007406	34.227149
944.920319	87430.401283	34.232167
945.656494	87566.432983	34.237184
946.620109	87715.140931	34.242202
947.562206	87861.853691	34.247220
948.936570	87992.403412	34.252237
949.467286	88151.139852	34.257255
950.543580	88298.668443	34.262272
951.607128	88436.201410	34.267290
952.187568	88570.163640	34.272308
953.051395	88697.093286	34.277325
953.943990	88835.878202	34.282343
954.927046	88977.003132	34.287360
955.888229	89110.740899	34.292378
956.717131	89260.018709	34.297396
957.887109	89398.026921	34.302413
958.622709	89540.639005	34.307431
959.530421	89687.495274	34.312448
960.463799	89829.601728	34.317466
960.859004	89981.506195	34.322484
961.900728	90137.317107	34.327501
963.021580	90289.736394	34.332519
963.719632	90447.941462	34.337536
965.059891	90601.066907	34.342554
965.696399	90767.612993	34.347572
966.750398	90931.958344	34.352589
967.938435	91080.700756	34.357607
968.803073	91238.269552	34.362624
969.850719	91397.372383	34.367642
970.676936	91566.544470	34.372660
972.058184	91723.037326	34.377677
973.111752	91880.414501	34.382695
973.985100	92039.575688	34.387712
975.172292	92189.685832	34.392730
976.031984	92362.187111	34.397748
976.884981	92511.348148	34.402765
977.666010	92677.098614	34.407783
978.594365	92838.369937	34.412800
980.025545	93004.572103	34.417818
980.572299	93182.542616	34.422836
981.692860	93333.215155	34.427853
982.861607	93499.989438	34.432871
983.878300	93661.916188	34.437888
985.281019	93809.620711	34.442906
986.116186	93987.802561	34.447924
986.968274	94143.240105	34.452941
988.207451	94302.083344	34.457959
989.190900	94456.583324	34.462976
990.021019	94619.534685	34.467994
990.980756	94789.947644	34.473012
991.963931	94950.021084	34.478029
992.975494	95113.566033	34.483047
994.000818	95284.477954	34.488064
995.102202	95443.528560	34.493082
995.950887	95612.376693	34.498100
997.204661	95772.936101	34.503117
997.962593	95939.237745	34.508135
998.695540	96106.380224	34.513152
999.837892	96271.683642	34.518170
1000.818498	96442.952757	34.523188
1001.759126	96617.268239	34.528205
1002.591374	96789.767035	34.533223
1003.497565	96967.395133	34.538240
1004.733118	97136.107310	34.543258
1005.353017	97315.760336	34.548276
1006.655633	97488.667284	34.553293
1007.611385	97656.473306	34.558311
1008.292062	97840.703418	34.563328
1009.714160	98008.441003	34.568346
1011.107880	98179.925883	34.573364
1011.822687	98349.814873	34.578381
1012.913413	98529.386036	34.583399
1013.852892	98703.159051	34.588416
1015.150793	98866.174693	34.593434
1015.972438	99043.559173	34.598452
1017.120795	99209.026515	34.603469
1018.074632	99374.071263	34.608487
1018.965800	99542.875463	34.613504
1020.474278	99688.482665	34.618522
1021.493679	99852.557340	34.623540
1022.712282	100004.304884	34.628557
1023.661882	100154.666946	34.633575
1024.390267	100317.545471	34.638592
1025.373984	100465.681432	34.643610
1026.216420	100628.245501	34.648628
1027.480949	100779.312592	34.653645
1028.551535	100938.042048	34.658663
1028.873250	101110.888926	34.663680
1030.397734	101275.914905	34.668698
1031.215386	101446.098760	34.673716
1032.036445	101605.038212	34.678733
1033.180396	101772.884553	34.683751
1034.244622	101944.360571	34.688768
1035.129215	102123.680806	34.693786
1036.354482	102291.149825	34.698804
1037.292872	102470.254615	34.703821
1038.623291	102649.555425	34.708839
1039.389769	102817.838204	34.713856
1040.451084	102989.625548	34.718874
1041.441763	103172.665011	34.723892
1042.573258	103351.560312	34.728909
1043.499630	103528.097226	34.733927
1044.666129	103713.777222	34.738944
1045.594776	103896.585063	34.743962
1046.454489	104077.239957	34.748980
1047.753797	104249.059554	34.753997
1048.837858	104439.862132	34.759015
1049.519056	104619.207823	34.764032
1051.018212	104810.666345	34.769050
1052.101067	104988.985615	34.774068
1053.039812	105182.059284	34.779085
1054.378217	105370.559517	34.784103
1055.290030	105555.002789	34.789120
1056.456179	105731.818812	34.794138
1057.666310	105914.556115	34.799156
1058.622950	106100.692925	34.804173
1059.680624	106282.622052	34.809191
1060.823281	106471.757757	34.814208
1062.048960	106653.598312	34.819226
1063.055203	106830.600072	34.824244
1064.184047	107016.575485	34.829261
1065.588169	107192.158607	34.834279
1066.427744	107375.372507	34.839296
1067.579869	107551.607621	34.844314
1068.514438	107731.844382	34.849332
1069.849009	107908.330328	34.854349
1070.960975	108095.265985	34.859367
1071.897061	108272.516857	34.864384
1072.898077	108449.365496	34.869402
1073.974065	108640.262836	34.874420
1074.718943	108830.101601	34.879437
1075.936507	109000.445357	34.884455
1076.893038	109195.673072	34.889472
1078.314148	109371.115587	34.894490
1078.924122	109565.440573	34.899508
1080.016891	109751.985502	34.904525
1081.152902	109930.911561	34.909543
1082.055667	110138.226789	34.914560
1083.175860	110323.263682	34.919578
1084.178295	110520.532753	34.924596
1085.408486	110706.339434	34.929613
1086.360492	110901.947470	34.934631
1087.067148	111093.037074	34.939648
1088.210768	111301.170017	34.944666
1089.438418	111489.997368	34.949684
1090.543548	111667.318372	34.954701
1091.743106	111853.036522	34.959719
1092.340971	112042.149132	34.964736
1093.533439	112223.399072	34.969754
1094.717126	112409.148916	34.974772
1095.294678	112606.769205	34.979789
1097.018838	112790.215262	34.984807
1097.399329	112995.687381	34.989824
1098.709827	113185.716113	34.994842
1099.841500	113379.056925	34.999860
1100.468155	113590.675098	35.004877
1101.709028	113789.055580	35.009895
1103.165431	114003.440884	35.014912
1104.495859	114191.978209	35.019930
1105.475716	114394.498271	35.024948
1106.720085	114598.711759	35.029965
1107.998511	114803.541899	35.034983
1108.867592	115010.519010	35.040000
1109.708834	115208.202735	35.045018
1110.926396	115422.536975	35.050036
1111.853599	115624.555108	35.055053
1113.167385	115842.196102	35.060071
1114.070486	116052.608743	35.065088
1115.231896	116264.107870	35.070106
1116.686924	116475.091226	35.075124
1117.441626	116699.318340	35.080141
1118.900446	116908.758498	35.085159
1119.602352	117136.976269	35.090176
1120.828278	117343.417195	35.095194
1122.289495	117560.185306	35.100212
1123.243482	117780.840140	35.105229
1124.690340	117996.144101	35.110247
1125.764131	118224.727153	35.115264
1126.784873	118431.209798	35.120282
1128.268921	118647.880940	35.125300
1129.372710	118869.469654	35.130317
1130.777039	119067.340328	35.135335
1131.347186	119300.564134	35.140352
1132.590422	119514.696584	35.145370
1133.895415	119728.465590	35.150388
1135.003201	119948.718663	35.155405
1136.143534	120159.210726	35.160423
1137.080370	120388.593721	35.165440
1138.175075	120619.080214	35.170458
1139.472260	120833.770957	35.175476
1140.739136	121063.763601	35.180493
1142.230629	121278.514165	35.185511
1143.201991	121497.597526	35.190528
1144.289706	121718.374054	35.195546
1145.935173	121926.311422	35.200564
1146.539513	122154.914045	35.205581
1147.719365	122373.525861	35.210599
1149.082112	122584.860181	35.215616
1150.280483	122808.490568	35.220634
1151.451744	123021.557809	35.225652
1152.296692	123244.020598	35.230669
1153.504484	123462.002101	35.235687
1154.238992	123690.594943	35.240704
1155.792662	123918.192304	35.245722
1156.980655	124138.222396	35.250740
1158.168391	124362.347703	35.255757
1159.466959	124579.308394	35.260775
1160.148383	124802.633508	35.265792
1161.318916	125022.863025	35.270810
1162.666164	125252.583064	35.275828
1163.828619	125481.714358	35.280845
1165.035246	125696.797120	35.285863
1165.924348	125926.610651	35.290880
1167.205308	126139.554968	35.295898
1168.521452	126361.696572	35.300916
1169.271226	126571.537750	35.305933
1170.468313	126780.609308	35.310951
1171.690645	127006.636831	35.315968
1172.641369	127219.922067	35.320986
1173.977229	127441.789358	35.326004
1174.927983	127667.486364	35.331021
1176.149832	127880.427130	35.336039
1177.545197	128117.195266	35.341056
1178.089181	128344.016469	35.346074
1179.839459	128563.161463	35.351092
1180.557739	128801.162155	35.356109
1181.862878	129027.811790	35.361127
1183.046844	129267.995283	35.366144
1184.230306	129495.961327	35.371162
1185.601330	129734.913276	35.376180
1186.608633	129968.679349	35.381197
1187.774888	130204.550439	35.386215
1189.091729	130449.512491	35.391232
1189.920859	130694.214806	35.396250
1191.357813	130929.793021	35.401268
1192.493486	131177.161098	35.406285
1193.607250	131420.592338	35.411303
1194.788526	131677.920459	35.416320
1196.030493	131926.189478	35.421338
1197.411090	132168.061093	35.426356
1198.511985	132419.818007	35.431373
1199.994188	132670.651822	35.436391
1201.540142	132918.231723	35.441408
1201.982781	133160.760250	35.446426
1203.339947	133400.832152	35.451444
1204.379974	133659.112206	35.456461
1205.561180	133918.131618	35.461479
1207.083984	134174.801986	35.466496
1208.006833	134430.052232	35.471514
1209.533448	134688.450163	35.476532
1210.501522	134944.850619	35.481549
1211.965213	135195.440718	35.486567
1213.308217	135466.261466	35.491584
1214.360245	135709.684366	35.496602
1215.787564	135962.403553	35.501620
1216.938570	136221.509508	35.506637
1218.253858	136479.753552	35.511655
1219.454847	136743.964725	35.516672
1220.372748	136992.477934	35.521690
1222.007873	137251.093476	35.526708
1223.092978	137506.530803	35.531725
1224.260713	137764.859886	35.536743
1225.671014	138032.761549	35.541760
1226.945962	138283.558234	35.546778
1228.731007	138530.684247	35.551796
1229.887966	138790.645904	35.556813
1230.915492	139042.896519	35.561831
1232.414199	139291.711054	35.566848
1233.427664	139553.097005	35.571866
1235.109874	139800.705720	35.576884
1236.023626	140057.192297	35.581901
1237.483946	140309.114450	35.586919
1238.472225	140555.030103	35.591936
1239.523043	140815.988389	35.596954
1241.122976	141057.951787	35.601972
1241.884424	141317.097711	35.606989
1243.493595	141562.841822	35.612007
1244.617774	141822.819186	35.617024
1245.796076	142078.896628	35.622042
1247.073021	142332.081146	35.627060
1248.009962	142591.359712	35.632077
1249.432589	142828.267091	35.637095
1250.620665	143069.437569	35.642112
1251.879152	143317.268244	35.647130
1253.146835	143551.746002	35.652148
1254.190956	143800.389048	35.657165
1255.298673	144038.409147	35.662183
1256.611593	144293.884442	35.667200
1257.888594	144539.108260	35.672218
1259.167981	144779.932897	35.677236
1260.449345	145044.828451	35.682253
1261.570990	145301.471237	35.687271
1263.178970	145544.859129	35.692288
1264.423828	145812.467597	35.697306
1265.485301	146060.958643	35.702324
1266.771246	146317.074233	35.707341
1268.226813	146568.331714	35.712359
1268.977063	146822.129819	35.717376
1270.394259	147088.374918	35.722394
1271.812575	147344.272952	35.727412
1272.681652	147617.296123	35.732429
1274.284589	147885.532841	35.737447
1275.421416	148142.142471	35.742464
1276.619920	148422.194094	35.747482
1278.110422	148691.152818	35.752500
1279.393330	148959.754641	35.757517
1280.334787	149230.114374	35.762535
1282.246726	149509.625070	35.767552
1283.227451	149781.288676	35.772570
1284.645763	150048.950102	35.777588
1286.279809	150326.128380	35.782605
1287.704171	150598.396802	35.787623
1288.822394	150866.823934	35.792640
1289.756122	151145.062582	35.797658
1291.289929	151409.150476	35.802676
1292.489675	151681.349671	35.807693
1294.007734	151958.825457	35.812711
1295.293798	152230.735264	35.817728
1296.253556	152518.898572	35.822746
1298.030793	152793.762700	35.827764
1298.913701	153076.361836	35.832781
1300.245536	153357.430134	35.837799
1301.873391	153619.374066	35.842816
1302.957478	153919.387294	35.847834
1304.287413	154190.948509	35.852852
1305.757223	154479.980797	35.857869
1306.976097	154756.790435	35.862887
1308.460364	155033.837233	35.867904
1309.274138	155329.681878	35.872922
1311.046611	155601.331947	35.877940
1312.474164	155886.170103	35.882957
1313.556617	156161.730955	35.887975
1315.136872	156446.725492	35.892992
1316.176903	156737.456406	35.898010
1317.909844	157009.794979	35.903028
1318.850917	157291.831282	35.908045
1320.440042	157580.498595	35.913063
1321.861501	157864.920556	35.918080
1322.959638	158151.440397	35.923098
1324.262880	158420.535816	35.928116
1325.659112	158709.674396	35.933133
1327.131999	158996.633018	35.938151
1328.449928	159273.647840	35.943168
1330.021286	159557.841199	35.948186
1331.364740	159828.664598	35.953204
1332.635051	160119.026466	35.958221
1334.100601	160392.802042	35.963239
1335.542731	160664.984772	35.968256
1336.613005	160934.947120	35.973274
1338.555460	161191.839132	35.978292
1339.175195	161448.545359	35.983309
1340.699786	161712.309842	35.988327
1341.839615	161974.680557	35.993344
1342.934277	162246.956384	35.998362
1344.194556	162500.480172	36.003380
1345.771904	162765.663501	36.008397
1346.740906	163035.960567	36.013415
1348.168548	163311.258553	36.018432
1349.173905	163590.586637	36.023450
1350.968873	163869.938292	36.028468
1352.337575	164151.481072	36.033485
1353.360339	164422.310885	36.038503
1354.904402	164698.727740	36.043520
1355.903681	164995.372267	36.048538
1357.381607	165276.143030	36.053556
1358.534218	165566.663133	36.058573
1360.016060	165858.488396	36.063591
1361.181769	166142.209242	36.068608
1362.586268	166451.269310	36.073626
1364.050107	166736.302368	36.078644
1365.272878	167034.738195	36.083661
1366.449096	167341.317166	36.088679
1368.142393	167637.217662	36.093696
1369.515809	167947.536767	36.098714
1370.879561	168241.034075	36.103732
1372.180778	168543.679728	36.108749
1373.480547	168858.014319	36.113767
1374.942990	169151.120551	36.118784
1376.126467	169472.533806	36.123802
1377.596801	169783.445870	36.128820
1379.186858	170095.723407	36.133837
1380.706861	170405.489424	36.138855
1382.238582	170709.976698	36.143872
1383.873233	171027.062536	36.148890
1384.901903	171326.421522	36.153908
1386.671253	171636.192616	36.158925
1387.905174	171943.668536	36.163943
1389.414076	172245.415883	36.168960
1390.895340	172560.545122	36.173978
1392.520872	172856.896488	36.178996
1393.838843	173169.252225	36.184013
1395.046219	173482.021688	36.189031
1396.500635	173777.429900	36.194048
1397.781282	174097.551733	36.199066
1399.475529	174398.685629	36.204084
1401.011588	174707.918826	36.209101
1402.449371	175021.954658	36.214119
1403.748966	175314.897766	36.219136
1404.923953	175630.440390	36.224154
1406.676898	175935.559043	36.229172
1408.092721	176242.385141	36.234189
1409.533571	176559.438093	36.239207
1411.076465	176854.063455	36.244224
1412.303613	177169.848417	36.249242
1413.545673	177474.946742	36.254260
1415.071401	177781.548404	36.259277
1416.493763	178097.116564	36.264295
1418.021498	178393.212997	36.269312
1419.386289	178705.266184	36.274330
1420.650585	179018.150163	36.279348
1422.251813	179328.023169	36.284365
1423.508842	179648.705006	36.289383
1425.034525	179951.562911	36.294400
1426.550641	180266.811657	36.299418
1428.026803	180574.123616	36.304436
1429.553903	180883.104344	36.309453
1431.054182	181193.576328	36.314471
1432.243133	181468.194808	36.319488
1433.701383	181770.274773	36.324506
1435.151578	182059.068708	36.329524
1436.772232	182337.631192	36.334541
1437.914150	182638.384868	36.339559
1439.468688	182917.849787	36.344576
1440.694623	183224.329975	36.349594
1442.572145	183514.457343	36.354612
1443.885319	183802.788275	36.359629
1445.352282	184094.179721	36.364647
1446.716854	184382.264055	36.369664
1447.980532	184689.355519	36.374682
1449.493516	184982.686130	36.379700
1450.719048	185283.364435	36.384717
1452.185145	185590.922490	36.389735
1453.880655	185893.862006	36.394752
1455.272846	186201.461021	36.399770
1456.517761	186524.927622	36.404788
1458.255334	186830.835527	36.409805
1459.447468	187156.116949	36.414823
1460.900172	187467.673278	36.419840
1462.332269	187772.862397	36.424858
1463.976960	188108.216824	36.429876
1465.782632	188412.268614	36.434893
1466.764442	188741.795466	36.439911
1468.309645	189045.487398	36.444928
1469.899570	189365.714042	36.449946
1470.995268	189691.673042	36.454964
1472.728129	190007.360395	36.459981
1473.886066	190343.138103	36.464999
1475.591733	190666.285056	36.470016
1477.155779	190996.350286	36.475034
1478.443377	191329.598573	36.480052
1480.072346	191646.543100	36.485069
1481.535837	191987.255789	36.490087
1483.311645	192311.453597	36.495104
1484.719875	192633.301827	36.500122
1486.562513	192962.925428	36.505140
1488.040983	193286.390400	36.510157
1489.698375	193623.779375	36.515175
1491.184198	193942.625518	36.520192
1492.990100	194269.558013	36.525210
1493.934012	194592.229371	36.530228
1495.627913	194920.186651	36.535245
1497.099997	195245.757443	36.540263
1498.545451	195581.516049	36.545280
1499.810156	195902.249362	36.550298
1501.356864	196237.854986	36.555316
1503.314774	196558.108812	36.560333
1504.759898	196899.892008	36.565351
1506.162888	197217.752374	36.570368
1507.532769	197561.722399	36.575386
1508.924727	197895.013283	36.580404
1510.996674	198225.374956	36.585421
1512.308745	198561.018398	36.590439
1513.887685	198889.522283	36.595456
1515.453076	199216.633410	36.600474
1516.909544	199541.783485	36.605492
1518.491581	199876.246110	36.610509
1519.894049	200215.247221	36.615527
1521.884210	200544.465516	36.620544
1523.111979	200873.773238	36.625562
1524.128583	201207.599259	36.630580
1525.945363	201528.496481	36.635597
1527.255285	201871.355204	36.640615
1528.920611	202202.171153	36.645632
1530.421011	202537.637489	36.650650
1531.908726	202864.689480	36.655668
1533.566587	203175.221587	36.660685
1535.204606	203496.588760	36.665703
1536.717332	203800.938688	36.670720
1537.987767	204128.603551	36.675738
1539.566190	204436.398810	36.680756
1541.267180	204750.345885	36.685773
1542.895670	205073.943410	36.690791
1544.212571	205383.880770	36.695808
1545.809750	205702.864338	36.700826
1547.378646	206031.960990	36.705844
1549.191369	206345.781871	36.710861
1550.401190	206671.982066	36.715879
1551.907364	206998.045770	36.720896
1553.511490	207312.666834	36.725914
1554.630022	207642.428740	36.730932
1556.238523	207966.993892	36.735949
1557.768771	208313.692698	36.740967
1559.131709	208640.218484	36.745984
1561.307385	208987.448413	36.751002
1562.270862	209325.420179	36.756020
1564.379921	209662.797716	36.761037
1565.727823	210008.264010	36.766055
1567.563039	210349.156112	36.771072
1569.276992	210691.821960	36.776090
1570.316681	211043.006752	36.781108
1572.348099	211382.270614	36.786125
1574.091652	211729.354689	36.791143
1575.501046	212068.495442	36.796160
1576.975680	212413.925101	36.801178
1578.718196	212763.070573	36.806196
1580.234844	213105.778536	36.811213
1581.684714	213456.473487	36.816231
1583.559992	213799.353414	36.821248
1585.162422	214147.613115	36.826266
1586.541644	214497.130084	36.831284
1588.497816	214845.867325	36.836301
1590.248916	215206.754332	36.841319
1591.590452	215559.075230	36.846336
1593.466719	215908.616945	36.851354
1594.739945	216258.996106	36.856372
1596.619609	216612.019314	36.861389
1598.193575	216959.354385	36.866407
1599.931694	217320.505476	36.871424
1601.341510	217670.587767	36.876442
1603.059219	218023.388821	36.881460
1604.634756	218370.906367	36.886477
1606.088549	218737.265397	36.891495
1607.998600	219086.406413	36.896512
1609.308632	219444.334037	36.901530
1610.660428	219803.195741	36.906548
1612.758400	220145.756423	36.911565
1614.647355	220517.866130	36.916583
1615.840902	220870.255502	36.921600
1617.890899	221220.878997	36.926618
1619.431416	221584.947682	36.931636
1621.131790	221941.320629	36.936653
1622.994227	222292.054722	36.941671
1624.590908	222642.630622	36.946688
1626.042576	222992.799775	36.951706
1627.598487	223351.359990	36.956724
1629.360845	223699.067020	36.961741
1630.821757	224060.769258	36.966759
1632.297429	224396.511714	36.971776
1633.818621	224785.256843	36.976794
1635.538608	225194.645841	36.981812
1637.061564	225554.081748	36.986829
1638.450773	225913.540800	36.991847
1639.982190	226273.282195	36.996864
1641.795592	226622.030581	37.001882
1643.062408	226968.533403	37.006900
1645.131018	227301.163161	37.011917
1646.329771	227647.044037	37.016935
1647.739614	227994.211769	37.021952
1649.500407	228345.335700	37.026970
1650.825759	228700.698167	37.031988
1652.714211	229062.013875	37.037005
1654.155771	229420.305478	37.042023
1655.665844	229786.841914	37.047040
1657.538815	230149.280626	37.052058
1659.072422	230511.014293	37.057076
1660.781328	230893.675654	37.062093
1662.085971	231259.741754	37.067111
1663.680921	231646.818256	37.072128
1665.339912	232018.187289	37.077146
1666.805668	232406.912737	37.082164
1668.451095	232795.126852	37.087181
1670.009201	233183.661163	37.092199
1671.501004	233584.603229	37.097216
1673.282950	233974.728152	37.102234
1674.955321	234377.826848	37.107252
1676.765162	234779.532119	37.112269
1678.496649	235183.842240	37.117287
1679.860730	235590.449341	37.122304
1681.832832	235996.550506	37.127322
1683.278452	236406.702234	37.132340
1685.047889	236813.270534	37.137357
1687.010767	237219.756960	37.142375
1688.607764	237638.802445	37.147392
1690.541496	238044.355558	37.152410
1692.119474	238456.826819	37.157428
1694.322225	238874.479350	37.162445
1696.032274	239285.711169	37.167463
1697.324619	239699.807032	37.172480
1699.544942	240102.649622	37.177498
1700.813973	240529.807664	37.182516
1702.611468	240933.991720	37.187533
1704.757535	241352.115613	37.192551
1706.249110	241770.627790	37.197568
1708.120143	242176.529192	37.202586
1710.153554	242599.170090	37.207604
1711.832310	243007.644850	37.212621
1713.022709	243419.960503	37.217639
1715.058763	243842.933214	37.222656
1716.942368	244257.675892	37.227674
1718.529639	244673.077792	37.232692
1720.708159	245086.833051	37.237709
1722.070471	245501.206358	37.242727
1723.756356	245912.757863	37.247744
1725.746701	246329.441784	37.252762
1727.360180	246749.465451	37.257780
1729.154759	247172.990721	37.262797
1731.378089	247581.915201	37.267815
1732.841743	247997.494178	37.272832
1734.967237	248401.075689	37.277850
1736.660254	248812.476963	37.282868
1738.279750	249228.209304	37.287885
1740.221396	249634.921555	37.292903
1741.934366	250034.584486	37.297920
1743.932087	250437.223689	37.302938
1745.522765	250849.558235	37.307956
1747.542150	251254.201352	37.312973
1749.277816	251663.337183	37.317991
1750.937600	252070.860032	37.323008
1752.917607	252454.019407	37.328026
1754.425808	252861.593203	37.333044
1756.349956	253257.895712	37.338061
1758.304467	253633.159542	37.343079
1759.677901	254014.717916	37.348096
1761.418603	254383.869813	37.353114
1763.018712	254775.018895	37.358132
1764.664427	255148.022656	37.363149
1766.193313	255528.488994	37.368167
1767.527339	255925.702989	37.373184
1769.600687	256317.003023	37.378202
1771.227646	256705.226870	37.383220
1773.122977	257114.059342	37.388237
1774.851751	257512.605648	37.393255
1776.338987	257910.556812	37.398272
1778.236362	258315.553188	37.403290
1779.497934	258722.737665	37.408308
1781.272368	259132.580987	37.413325
1782.841151	259548.529647	37.418343
1784.401658	259974.666360	37.423360
1786.444140	260395.693555	37.428378
1788.530127	260830.355057	37.433396
1790.127088	261252.446394	37.438413
1791.964324	261673.583416	37.443431
1793.749215	262110.504382	37.448448
1795.432045	262538.500098	37.453466
1796.910857	262979.891445	37.458484
1799.396724	263412.275930	37.463501
1801.151140	263846.025766	37.468519
1802.850299	264287.786500	37.473536
1805.032595	264724.970804	37.478554
1806.561848	265161.348170	37.483572
1808.363099	265612.642768	37.488589
1810.030817	266055.118783	37.493607
1811.644580	266493.919903	37.498624
1813.641605	266938.373050	37.503642
1815.212326	267402.532778	37.508660
1817.266804	267865.138771	37.513677
1819.133057	268315.404101	37.518695
1820.884505	268773.842273	37.523712
1822.937749	269212.085533	37.528730
1824.919991	269676.606654	37.533748
1826.660237	270138.779288	37.538765
1828.474154	270591.616305	37.543783
1830.461417	271061.316974	37.548800
1832.568733	271514.764762	37.553818
1834.367562	271973.190988	37.558836
1836.061040	272425.791303	37.563853
1837.907373	272882.074474	37.568871
1839.413709	273345.881448	37.573888
1841.615686	273805.508346	37.578906
1843.027119	274270.015299	37.583924
1845.143143	274734.506671	37.588941
1847.218994	275199.029232	37.593959
1848.725240	275670.605251	37.598976
1850.818337	276133.853061	37.603994
1852.796520	276608.778589	37.609012
1854.243364	277078.812038	37.614029
1856.605670	277534.976114	37.619047
1858.142526	278021.427895	37.624064
1860.023428	278482.368849	37.629082
1862.054642	278950.929958	37.634100
1863.960254	279418.545445	37.639117
1865.670871	279888.808420	37.644135
1867.675665	280362.476314	37.649152
1869.664972	280824.765578	37.654170
1871.677658	281294.721138	37.659188
1873.310342	281756.889123	37.664205
1875.551874	282227.236265	37.669223
1877.413930	282694.774430	37.674240
1879.289466	283144.121651	37.679258
1880.890861	283582.082318	37.684276
1882.579788	284032.855018	37.689293
1884.727468	284467.903535	37.694311
1886.366204	284910.325040	37.699328
1888.511451	285356.903622	37.704346
1890.389824	285796.057074	37.709364
1891.635436	286246.998175	37.714381
1893.813799	286686.074067	37.719399
1895.446351	287152.697020	37.724416
1897.444671	287608.665960	37.729434
1899.078576	288067.868683	37.734452
1900.908099	288533.870327	37.739469
1903.206073	289004.796909	37.744487
1905.033779	289475.266097	37.749504
1906.879910	289939.837711	37.754522
1908.734964	290410.553040	37.759540
1910.158402	290884.868534	37.764557
1912.117248	291362.243435	37.769575
1914.141940	291845.879408	37.774592
1915.990996	292327.485102	37.779610
1918.034000	292801.817948	37.784628
1919.903561	293302.669313	37.789645
1921.618401	293792.800127	37.794663
1923.497116	294293.721939	37.799680
1925.543451	294785.343157	37.804698
1927.783388	295279.952764	37.809716
1929.449452	295783.062020	37.814733
1931.183730	296277.801471	37.819751
1932.968735	296788.252140	37.824768
1935.322285	297295.253867	37.829786
1937.682280	297802.506084	37.834804
1939.093347	298301.124679	37.839821
1941.343466	298802.243730	37.844839
1943.003802	299334.443467	37.849856
1945.218534	299839.296749	37.854874
1947.340094	300364.531962	37.859892
1949.039535	300873.833471	37.864909
1951.024732	301381.739038	37.869927
1953.119497	301900.671723	37.874944
1955.321614	302423.875982	37.879962
1957.024480	302931.972215	37.884980
1959.000380	303455.030233	37.889997
1961.312544	303964.899513	37.895015
1963.189121	304490.075903	37.900032
1965.174428	305018.405820	37.905050
1967.129555	305532.159977	37.910068
1969.013908	306063.979575	37.915085
1971.236562	306578.546824	37.920103
1973.387538	307106.227142	37.925120
1975.321619	307621.572192	37.930138
1977.256766	308141.027983	37.935156
1978.871431	308659.060482	37.940173
1981.180952	309188.275898	37.945191
1982.783383	309717.782369	37.950208
1984.559055	310244.107745	37.955226
1986.728318	310772.624774	37.960244
1988.687349	311312.346613	37.965261
1990.827750	311844.213238	37.970279
1993.044237	312376.038220	37.975296
1995.165500	312907.087984	37.980314
1997.141207	313444.024042	37.985332
1999.061147	313964.459474	37.990349
2001.374210	314493.257005	37.995367
2003.004109	315014.545484	38.000384
2005.238637	315546.954191	38.005402
2007.620424	316069.482128	38.010420
2009.292423	316595.729207	38.015437
2011.371416	317113.424000	38.020455
2013.247866	317616.750852	38.025472
2015.211167	318115.666834	38.030490
2017.140597	318616.387624	38.035508
2019.014528	319117.240853	38.040525
2021.286294	319624.956627	38.045543
2023.204534	320116.831805	38.050560
2024.904566	320635.705002	38.055578
2027.176608	321142.342688	38.060596
2028.773015	321658.000228	38.065613
2031.132657	322169.363560	38.070631
2033.058809	322678.255339	38.075648
2035.073423	323206.044265	38.080666
2036.748589	323719.793301	38.085684
2038.775389	324260.215668	38.090701
2040.918286	324786.345157	38.095719
2042.871689	325316.309870	38.100736
2044.731867	325840.598190	38.105754
2047.024641	326387.381424	38.110772
2048.804685	326932.543299	38.115789
2051.028895	327470.543453	38.120807
2053.280559	328019.273463	38.125824
2055.005900	328562.702973	38.130842
2057.119747	329107.459614	38.135860
2058.921220	329667.672995	38.140877
2060.760686	330221.020049	38.145895
2063.126774	330791.208003	38.150912
2064.669822	331354.697024	38.155930
2067.162211	331924.014893	38.160948
2069.067506	332499.415048	38.165965
2071.198880	333066.800653	38.170983
2073.360812	333648.645260	38.176000
2075.533956	334226.140863	38.181018
2078.022776	334797.130308	38.186036
2079.668632	335378.102222	38.191053
2082.155294	335953.928181	38.196071
2084.079453	336541.212956	38.201088
2086.223084	337122.337328	38.206106
2088.683921	337699.265262	38.211124
2090.520135	338282.737299	38.216141
2092.702586	338860.307368	38.221159
2094.867268	339440.285197	38.226176
2096.737174	340036.626115	38.231194
2098.668023	340612.364737	38.236212
2100.874548	341208.128443	38.241229
2103.094297	341796.699728	38.246247
2105.148946	342396.865172	38.251264
2106.952975	342993.384322	38.256282
2109.405763	343583.316886	38.261300
2111.320635	344194.599913	38.266317
2113.696224	344797.195144	38.271335
2115.450563	345392.195151	38.276352
2117.214426	346002.337669	38.281370
2119.648465	346612.970675	38.286388
2121.660808	347226.583828	38.291405
2123.541039	347840.591290	38.296423
2126.098761	348443.083833	38.301440
2127.757620	349066.145974	38.306458
2130.023082	349675.192472	38.311476
2132.143688	350299.988461	38.316493
2134.465159	350920.732974	38.321511
2136.557607	351540.922913	38.326528
2138.349144	352156.712942	38.331546
2140.953469	352779.414555	38.336564
2143.069010	353407.871989	38.341581
2144.586695	354024.822553	38.346599
2147.438734	354655.296994	38.351616
2149.100194	355274.844680	38.356634
2151.486019	355884.494736	38.361652
2153.475330	356503.640334	38.366669
2155.827106	357098.079554	38.371687
2157.946294	357685.292009	38.376704
2159.878078	358278.413426	38.381722
2162.332349	358879.736656	38.386740
2164.078371	359479.062056	38.391757
2166.208893	360082.881932	38.396775
2168.302725	360688.500123	38.401792
2170.310173	361305.819206	38.406810
2172.585074	361912.555927	38.411828
2174.744275	362536.503105	38.416845
2176.412759	363156.284680	38.421863
2179.009451	363774.863051	38.426880
2180.998303	364406.317622	38.431898
2183.405175	365033.938356	38.436916
2185.065302	365670.753700	38.441933
2187.627460	366310.580397	38.446951
2189.721747	366951.386709	38.451968
2191.623065	367590.894903	38.456986
2193.828100	368240.818161	38.462004
2196.118107	368894.064273	38.467021
2197.933259	369541.543252	38.472039
2200.235241	370199.685049	38.477056
2202.617719	370873.349909	38.482074
2204.784900	371534.964693	38.487092
2206.987546	372203.054466	38.492109
2209.537018	372871.454981	38.497127
2211.985047	373531.566249	38.502144
2213.781563	374200.598659	38.507162
2216.632139	374873.096403	38.512180
2218.815921	375540.593775	38.517197
2220.724331	376210.786638	38.522215
2223.416401	376882.612363	38.527232
2225.240884	377567.983262	38.532250
2227.808890	378231.358411	38.537268
2230.161343	378915.245729	38.542285
2232.286277	379590.763348	38.547303
2234.666058	380259.936730	38.552320
2236.758924	380951.686265	38.557338
2239.128031	381628.593128	38.562356
2241.237448	382312.983590	38.567373
2243.470078	382998.759370	38.572391
2245.891738	383679.494705	38.577408
2248.182240	384370.911537	38.582426
2251.036901	385054.867933	38.587444
2252.759100	385746.475860	38.592461
2255.072470	386428.869719	38.597479
2257.727933	387118.265680	38.602496
2259.430064	387807.626519	38.607514
2261.793256	388496.939211	38.612532
2264.142935	389189.585198	38.617549
2266.531596	389879.370182	38.622567
2268.912073	390577.176841	38.627584
2270.930520	391270.160528	38.632602
2273.478626	391964.283184	38.637620
2275.775347	392661.549263	38.642637
2278.077821	393353.551571	38.647655
2280.631130	394038.703811	38.652672
2282.937378	394746.362807	38.657690
2285.322858	395421.930433	38.662708
2287.348564	396110.847949	38.667725
2289.774869	396803.611602	38.672743
2291.879141	397486.300108	38.677760
2293.795996	398191.888099	38.682778
2296.939645	398866.668596	38.687796
2298.772784	399572.287561	38.692813
2300.970877	400268.655627	38.697831
2303.428222	400940.459949	38.702848
2305.869564	401618.560688	38.707866
2308.225259	402276.616155	38.712884
2310.073861	402934.816019	38.717901
2312.146529	403593.571625	38.722919
2314.536476	404266.803001	38.727936
2316.365508	404937.906408	38.732954
2318.659355	405609.068898	38.737972
2321.061853	406302.086989	38.742989
2323.257960	406986.761192	38.748007
2325.450893	407651.734130	38.753024
2327.734192	408347.684210	38.758042
2330.072241	409056.983164	38.763060
2332.527951	409754.945889	38.768077
2334.463487	410458.777258	38.773095
2336.656020	411160.926513	38.778112
2339.003613	411879.040355	38.783130
2341.159867	412586.249279	38.788148
2343.497271	413312.405974	38.793165
2345.897190	414051.880182	38.798183
2348.107771	414762.618078	38.803200
2350.114738	415505.839002	38.808218
2352.728573	416252.509386	38.813236
2355.060440	416983.249742	38.818253
2357.434969	417734.601702	38.823271
2360.013590	418472.932074	38.828288
2362.161463	419244.535857	38.833306
2364.735034	419980.797252	38.838324
2367.499957	420744.378054	38.843341
2369.461865	421504.523170	38.848359
2372.276043	422243.742073	38.853376
2374.344385	423013.698240	38.858394
2376.887684	423777.754087	38.863412
2379.359957	424537.544522	38.868429
2381.309659	425312.182594	38.873447
2384.377204	426075.067431	38.878464
2386.273998	426849.715794	38.883482
2388.740700	427611.588016	38.888500
2391.523032	428385.686358	38.893517
2393.654830	429165.233258	38.898535
2396.441002	429932.699377	38.903552
2399.037580	430716.522855	38.908570
2401.682339	431490.238810	38.913588
2404.018612	432268.181496	38.918605
2406.865800	433044.343571	38.923623
2409.407731	433803.422051	38.928640
2411.388793	434572.488477	38.933658
2414.181465	435343.925894	38.938676
2416.728375	436111.683339	38.943693
2419.029029	436883.200633	38.948711
2421.760206	437649.813024	38.953728
2424.092729	438419.349715	38.958746
2426.551336	439177.099287	38.963764
2428.848531	439957.519503	38.968781
2431.177500	440734.415799	38.973799
2433.283692	441497.002396	38.978816
2435.743876	442282.626919	38.983834
2438.298090	443055.964005	38.988852
2440.635812	443838.618659	38.993869
2442.945431	444622.514695	38.998887
2445.541100	445401.428129	39.003904
2448.233317	446189.403364	39.008922
2450.508139	446969.375580	39.013940
2453.050080	447754.384358	39.018957
2455.406600	448535.651861	39.023975
2457.949790	449302.899812	39.028992
2460.163750	450092.125278	39.034010
2462.599240	450872.990191	39.039028
2464.828720	451649.662433	39.044045
2467.321681	452428.184163	39.049063
2469.947185	453178.234236	39.054080
2472.150207	453927.972963	39.059098
2474.387432	454693.000711	39.064116
2476.923915	455443.792444	39.069133
2479.018185	456222.844018	39.074151
2481.392582	456990.847886	39.079168
2483.878659	457760.220041	39.084186
2486.412489	458543.054002	39.089204
2488.696944	459326.202121	39.094221
2491.373639	460113.147678	39.099239
2493.569638	460894.631538	39.104256
2496.373964	461683.465786	39.109274
2499.125693	462480.567227	39.114292
2501.472718	463271.587359	39.119309
2503.921944	464077.873599	39.124327
2506.540709	464880.409266	39.129344
2508.981666	465675.259387	39.134362
2511.095432	466487.465373	39.139380
2514.164539	467297.508898	39.144397
2516.405472	468113.769631	39.149415
2518.630402	468935.405224	39.154432
2521.549344	469763.358801	39.159450
2523.875583	470587.786916	39.164468
2526.424926	471429.118667	39.169485
2529.003092	472261.971152	39.174503
2531.837648	473085.752076	39.179520
2534.206101	473925.638403	39.184538
2536.992023	474763.397586	39.189556
2539.527576	475600.604814	39.194573
2541.865795	476448.161581	39.199591
2544.947974	477282.677156	39.204608
2547.801927	478129.213060	39.209626
2550.399742	478983.428767	39.214644
2553.436616	479806.928279	39.219661
2555.688596	480650.063233	39.224679
2558.632478	481479.006762	39.229696
2561.182130	482317.015835	39.234714
2563.719903	483152.867206	39.239732
2566.524599	483982.223398	39.244749
2569.012749	484826.891016	39.249767
2571.794553	485653.547932	39.254784
2574.310900	486489.801824	39.259802
2576.562219	487329.643966	39.264820
2579.695456	488167.483345	39.269837
2582.066514	489006.216040	39.274855
2584.791705	489843.790118	39.279872
2587.715844	490678.363775	39.284890
2590.013365	491516.230604	39.289908
2593.069147	492342.223665	39.294925
2595.328950	493189.301127	39.299943
2597.990310	494017.801865	39.304960
2600.421736	494859.318618	39.309978
2603.091561	495698.786673	39.314996
2605.891644	496537.687162	39.320013
2608.632670	497377.110711	39.325031
2611.049165	498209.331845	39.330048
2613.871575	499054.812879	39.335066
2616.002579	499898.448372	39.340084
2619.102310	500735.172726	39.345101
2621.382524	501583.439545	39.350119
2624.231917	502421.078374	39.355136
2627.118834	503252.313876	39.360154
2629.335350	504107.925352	39.365172
2632.375264	504941.016760	39.370189
2634.802518	505791.613783	39.375207
2637.341418	506627.121941	39.380224
2639.772791	507448.789646	39.385242
2642.390448	508272.804817	39.390260
2645.234653	509072.994980	39.395277
2647.815188	509884.430642	39.400295
2650.326912	510680.360618	39.405312
2653.148716	511493.690985	39.410330
2655.748142	512303.135181	39.415348
2658.367519	513098.623667	39.420365
2660.711601	513926.977935	39.425383
2663.061090	514735.380873	39.430400
2665.918069	515549.756076	39.435418
2668.631697	516389.005887	39.440436
2671.098759	517207.692424	39.445453
2673.815778	518051.034131	39.450471
2676.001913	518887.666001	39.455488
2678.623118	519728.614161	39.460506
2681.447330	520576.132642	39.465524
2683.896769	521439.383011	39.470541
2686.537915	522297.817891	39.475559
2688.749578	523164.787533	39.480576
2691.415240	524035.309405	39.485594
2693.845542	524924.605465	39.490612
2696.818683	525803.082969	39.495629
2698.873491	526705.328489	39.500647
2701.920515	527599.853031	39.505664
2704.601069	528507.677019	39.510682
2707.300296	529411.917972	39.515700
2710.255582	530317.420682	39.520717
2712.947848	531235.949701	39.525735
2715.488427	532153.036759	39.530752
2718.435660	533061.945507	39.535770
2721.049137	533998.686546	39.540788
2724.252025	534927.267580	39.545805
2726.635359	535860.805830	39.550823
2729.659498	536784.163708	39.555840
2731.998605	537714.871582	39.560858
2734.937842	538654.929767	39.565876
2738.214325	539585.612803	39.570893
2740.719758	540530.297876	39.575911
2743.830530	541464.507335	39.580928
2746.231305	542404.104207	39.585946
2748.878801	543346.716232	39.590964
2752.254153	544286.277964	39.595981
2754.758884	545236.984536	39.600999
2757.470265	546177.383384	39.606016
2760.235464	547124.649102	39.611034
2763.247825	548071.557767	39.616052
2766.186132	549025.754331	39.621069
2769.031349	549979.447482	39.626087
2771.853686	550919.605052	39.631104
2774.854415	551859.417066	39.636122
2777.512159	552809.273708	39.641140
2780.164157	553756.250072	39.646157
2783.018666	554710.916631	39.651175
2785.859433	555660.241023	39.656192
2788.774949	556608.732138	39.661210
2791.313859	557559.479202	39.666228
2794.291432	558517.220694	39.671245
2797.125371	559470.294710	39.676263
2799.889886	560422.959889	39.681280
2802.830400	561373.116064	39.686298
2805.601976	562325.642436	39.691316
2808.481541	563274.314843	39.696333
2810.987808	564232.321186	39.701351
2814.003109	565196.801884	39.706368
2816.588634	566156.310535	39.711386
2819.116330	567118.569339	39.716404
2821.989520	568069.252141	39.721421
2824.838406	569025.240355	39.726439
2827.707247	569951.736963	39.731456
2830.744734	570871.512641	39.736474
2832.676095	571796.222725	39.741492
2835.823270	572713.738871	39.746509
2838.595256	573645.151577	39.751527
2841.259842	574570.591789	39.756544
2843.766538	575502.663522	39.761562
2846.816916	576456.652744	39.766580
2849.483667	577395.932555	39.771597
2852.149311	578357.565968	39.776615
2854.868372	579312.294001	39.781632
2857.609023	580271.208260	39.786650
2860.305759	581248.261261	39.791668
2863.001803	582220.773337	39.796685
2865.648827	583207.157019	39.801703
2868.588760	584195.468582	39.806720
2871.143951	585180.404102	39.811738
2874.118720	586191.210112	39.816756
2877.075964	587194.615581	39.821773
2880.097239	588204.092447	39.826791
2882.766522	589216.650094	39.831808
2885.870074	590236.768593	39.836826
2888.813957	591260.985629	39.841844
2891.489948	592280.849353	39.846861
2894.377261	593311.012234	39.851879
2897.315703	594353.501684	39.856896
2899.907168	595391.898399	39.861914
2902.953356	596447.810427	39.866932
2905.757779	597488.140291	39.871949
2908.737627	598549.883692	39.876967
2911.860331	599610.705358	39.881984
2914.749242	600665.910405	39.887002
2917.547520	601733.951587	39.892020
2920.646580	602802.044351	39.897037
2924.152835	603867.968199	39.902055
2926.789370	604933.986159	39.907072
2930.027756	606001.406780	39.912090
2932.683009	607081.434532	39.917108
2935.830478	608142.763355	39.922125
2939.069341	609218.887804	39.927143
2941.782811	610287.741537	39.932160
2945.005101	611358.860754	39.937178
2947.698060	612438.218036	39.942196
2950.964278	613532.080908	39.947213
2954.079001	614610.757676	39.952231
2956.808485	615695.593592	39.957248
2959.822444	616768.625643	39.962266
2962.789562	617862.109188	39.967284
2966.277755	618936.650976	39.972301
2969.373736	620014.750751	39.977319
2971.833544	621103.644676	39.982336
2974.734395	622171.216626	39.987354
2978.038694	623263.752383	39.992372
2981.124247	624349.318164	39.997389
2984.067421	625442.341963	40.002407
2986.920737	626533.021063	40.007424
2990.270179	627620.110322	40.012442
2992.832407	628717.407365	40.017460
2996.215344	629801.371159	40.022477
2999.181552	630893.132504	40.027495
3002.487103	631986.821966	40.032512
3005.388547	633068.182631	40.037530
3008.400964	634153.556804	40.042548
3011.447754	635240.359916	40.047565
3014.287769	636317.550933	40.052583
3017.423121	637407.706418	40.057600
3020.760362	638488.981402	40.062618
3023.485240	639551.334130	40.067636
3026.259423	640599.949298	40.072653
3029.293772	641638.387666	40.077671
3032.364772	642680.654974	40.082688
3035.656550	643706.221185	40.087706
3038.623352	644757.719184	40.092724
3041.421290	645793.728069	40.097741
3044.423011	646830.345038	40.102759
3047.497784	647889.676178	40.107776
3050.676530	648930.883310	40.112794
3053.637158	649986.572316	40.117812
3056.430585	651037.542412	40.122829
3059.356721	652094.060619	40.127847
3062.480522	653159.851140	40.132864
3065.423802	654223.563824	40.137882
3068.270149	655302.072926	40.142900
3071.214672	656386.674009	40.147917
3074.300913	657462.714771	40.152935
3077.447373	658566.166488	40.157952
3080.344806	659655.044376	40.162970
3083.222978	660765.411704	40.167988
3086.209236	661866.872315	40.173005
3089.828625	662974.922501	40.178023
3092.261926	664108.274810	40.183040
3095.544470	665227.070821	40.188058
3098.734133	666354.359863	40.193076
3101.657731	667484.395659	40.198093
3104.965851	668622.293071	40.203111
3107.861071	669764.847594	40.208128
3110.913638	670914.350431	40.213146
3114.051486	672070.860200	40.218164
3117.099712	673222.618264	40.223181
3120.291339	674380.227001	40.228199
3123.256944	675555.874159	40.233216
3126.759332	676715.876051	40.238234
3129.804448	677885.151793	40.243252
3132.897718	679057.601357	40.248269
3136.303836	680227.564917	40.253287
3139.474128	681397.915430	40.258304
3142.869443	682580.448209	40.263322
3146.030029	683753.728131	40.268340
3149.131934	684948.618012	40.273357
3152.335967	686123.075278	40.278375
3155.450045	687301.218044	40.283392
3158.860626	688489.036869	40.288410
3161.639894	689675.760817	40.293428
3164.797914	690866.632783	40.298445
3168.089770	692067.198894	40.303463
3171.465591	693261.884031	40.308480
3174.359745	694452.073081	40.313498
3177.474101	695644.099821	40.318516
3180.746030	696847.892182	40.323533
3184.128093	698052.146684	40.328551
3187.274213	699257.018812	40.333568
3190.524710	700467.012500	40.338586
3193.708435	701661.136864	40.343604
3196.588257	702880.324227	40.348621
3199.957115	704081.817088	40.353639
3202.888134	705304.421217	40.358656
3206.389623	706506.892880	40.363674
3209.900246	707720.042599	40.368692
3212.703665	708932.691605	40.373709
3216.001911	710137.956499	40.378727
3219.304872	711362.211155	40.383744
3222.465672	712580.619974	40.388762
3225.345829	713794.296690	40.393780
3228.649580	715006.343580	40.398797
3232.104264	716222.595204	40.403815
3234.769818	717445.776857	40.408832
3238.199997	718623.983802	40.413850
3241.389411	719800.728724	40.418868
3244.430047	720976.738414	40.423885
3247.958833	722145.726751	40.428903
3251.151431	723324.839648	40.433920
3254.294418	724497.959147	40.438938
3257.401805	725694.246641	40.443956
3260.374040	726873.678355	40.448973
3263.931513	728074.634405	40.453991
3266.867252	729266.672725	40.459008
3270.113939	730471.526143	40.464026
3273.025756	731675.317432	40.469044
3276.564750	732880.406504	40.474061
3279.971144	734104.445666	40.479079
3282.882725	735319.345798	40.484096
3286.133022	736539.830611	40.489114
3289.255824	737777.028802	40.494132
3292.864132	739015.978163	40.499149
3295.974037	740253.780490	40.504167
3298.757982	741524.740667	40.509184
3302.165481	742772.064633	40.514202
3305.479266	744025.568070	40.519220
3308.889697	745306.121677	40.524237
3312.537314	746582.285843	40.529255
3315.601130	747852.275049	40.534272
3318.868190	749131.239281	40.539290
3321.902584	750422.300216	40.544308
3325.123996	751717.006928	40.549325
3328.589274	753020.322439	40.554343
3332.129532	754323.700280	40.559360
3335.328628	755634.397323	40.564378
3338.997061	756937.407635	40.569396
3342.069563	758249.547375	40.574413
3345.412014	759567.567937	40.579431
3348.278820	760898.821640	40.584448
3352.013749	762221.039000	40.589466
3355.453916	763547.893271	40.594484
3358.561024	764894.436594	40.599501
3362.316953	766223.027595	40.604519
3365.633213	767566.252322	40.609536
3368.951459	768912.134264	40.614554
3372.640133	770242.869365	40.619572
3375.842759	771592.411373	40.624589
3379.417925	772929.805489	40.629607
3382.752295	774286.299098	40.634624
3386.357619	775631.005596	40.639642
3389.977720	776974.627440	40.644660
3392.845304	778316.701796	40.649677
3396.652725	779682.030366	40.654695
3399.853115	781029.388371	40.659712
3403.150985	782386.683843	40.664730
3406.958379	783741.775309	40.669748
3410.216153	785091.110326	40.674765
3413.824409	786457.932691	40.679783
3417.240574	787811.974202	40.684800
3420.295003	789171.356254	40.689818
3423.924367	790536.900762	40.694836
3427.244406	791898.998545	40.699853
3430.800147	793260.843150	40.704871
3434.012428	794639.034922	40.709888
3437.339611	796010.570657	40.714906
3440.940688	797392.366947	40.719924
3444.441654	798766.171480	40.724941
3447.493769	800135.618175	40.729959
3451.221691	801523.911855	40.734976
3454.686644	802895.092136	40.739994
3457.549459	804273.728244	40.745012
3460.915323	805647.304034	40.750016
3464.376000	806968.866899	40.755021
3467.628092	808243.651804	40.760026
3471.148569	809443.872947	40.765031
3474.562644	810600.788449	40.770036
3477.546164	811683.908847	40.775040
3480.765962	812689.535236	40.780045
3483.319009	813642.971084	40.785050
3486.152033	814506.871923	40.790055
3488.684613	815307.363044	40.795060
3490.824047	816059.852545	40.800064
3492.997022	816738.394400	40.805069
3495.455828	817357.700510	40.810074
3497.574686	817925.084005	40.815079
3499.490625	818421.598667	40.820084
3501.443873	818861.948462	40.825088
3503.604020	819254.923332	40.830093
3504.851552	819602.379527	40.835098
3506.472472	819897.654660	40.840103
3508.173689	820129.405644	40.845108
3509.018022	820340.841853	40.850112
3510.479304	820500.317646	40.855117
3512.025846	820621.718782	40.860122
3512.657062	820703.255593	40.865127
3514.100357	820758.781468	40.870132
3515.032303	820778.096203	40.875136
3516.006314	820762.087238	40.880141
3516.448401	820716.865514	40.885146
3517.685841	820652.386287	40.890151
3518.658767	820555.762867	40.895156
3518.989560	820440.508425	40.900160
3519.457846	820291.279825	40.905165
3520.225113	820126.882367	40.910170
3520.511609	819943.578626	40.915175
3521.392191	819749.849256	40.920180
3521.823335	819520.424653	40.925184
3522.219858	819281.750796	40.930189
3522.762994	819035.117885	40.935194
3522.960475	818769.890508	40.940199
3523.139554	818477.694073	40.945204
3523.275546	818199.193475	40.950208
3523.490634	817912.838408	40.955213
3523.939380	817604.508134	40.960218
3524.308446	817290.548547	40.965223
3524.489425	816959.230362	40.970228
3524.395053	816623.927561	40.975232
3524.526053	816287.689731	40.980237
3524.296379	815940.921082	40.985242
3524.700521	815602.547879	40.990247
3524.853594	815232.867280	40.995252
3524.463732	814876.425581	41.000256
3524.850360	814504.512164	41.005261
3524.959865	814142.073825	41.010266
3524.582606	813769.804901	41.015271
3524.824806	813401.232888	41.020276
3524.361028	813035.009712	41.025280
3524.797042	812648.342864	41.030285
3524.988691	812278.983131	41.035290
3524.695026	811897.927911	41.040295
3524.976433	811505.539326	41.045300
3524.722658	811110.081037	41.050304
3524.821093	810732.422434	41.055309
3524.848588	810341.771731	41.060314
3524.996620	809957.202907	41.065319
3525.157021	809554.873301	41.070324
3524.483607	809170.003195	41.075328
3524.703690	808772.909377	41.080333
3524.684572	808380.732326	41.085338
3524.371876	807983.141095	41.090343
3524.349392	807575.823584	41.095348
3524.100118	807201.309567	41.100352
3524.200223	806796.964176	41.105357
3524.166740	806410.558084	41.110362
3523.667306	806025.579531	41.115367
3524.218894	805625.404367	41.120372
3523.856433	805241.192509	41.125376
3523.939039	804852.914250	41.130381
3523.680876	804460.208073	41.135386
3523.470684	804073.502989	41.140391
3523.673989	803691.709985	41.145396
3523.162895	803298.292445	41.150400
3523.065683	802912.140908	41.155405
3523.220108	802534.215263	41.160410
3522.937279	802150.160606	41.165415
3522.994869	801757.346084	41.170420
3522.379454	801375.412345	41.175424
3522.417344	801011.795762	41.180429
3522.469715	800632.114739	41.185434
3522.476481	800250.359712	41.190439
3522.172730	799875.160619	41.195444
3521.738631	799506.145364	41.200448
3522.009969	799128.357627	41.205453
3521.481813	798767.022775	41.210458
3521.523910	798404.544541	41.215463
3521.338553	798040.956054	41.220468
3521.414427	797682.802681	41.225472
3521.223761	797320.404457	41.230477
3521.449210	796971.663142	41.235482
3520.981700	796603.333727	41.240487
3521.190450	796241.697221	41.245492
3520.653923	795886.203408	41.250496
3520.516816	795519.382474	41.255501
3520.233632	795181.927881	41.260506
3520.485941	794843.092134	41.265511
3520.518834	794480.853422	41.270516
3520.069647	794137.336009	41.275520
3520.048212	793783.958559	41.280525
3519.762785	793449.907684	41.285530
3519.499764	793113.577990	41.290535
3519.625196	792767.836103	41.295540
3519.204602	792451.196305	41.300544
3519.127271	792109.384962	41.305549
3518.922692	791789.634326	41.310554
3518.791369	791453.891355	41.315559
3518.279562	791131.164829	41.320564
3518.277478	790820.622042	41.325568
3518.383663	790501.105730	41.330573
3518.199673	790190.319563	41.335578
3518.172683	789871.484634	41.340583
3518.284854	789556.936622	41.345588
3517.841513	789249.640738	41.350592
3517.374941	788938.698782	41.355597
3517.379770	788634.988136	41.360602
3517.339002	788335.400372	41.365607
3517.600063	788030.638725	41.370612
3517.134867	787736.551211	41.375616
3517.129724	787431.955227	41.380621
3517.091609	787140.426985	41.385626
3516.786700	786840.819799	41.390631
3516.902738	786549.143652	41.395636
3516.447758	786271.904799	41.400640
3516.677402	785968.387459	41.405645
3516.475233	785682.873773	41.410650
3516.110520	785402.390531	41.415655
3516.278566	785116.793234	41.420660
3516.270175	784833.770519	41.425664
3516.001994	784544.141037	41.430669
3515.839797	784272.824719	41.435674
3515.939924	783993.832474	41.440679
3515.820247	783718.160585	41.445684
3515.635624	783452.423323	41.450688
3515.385062	783175.276732	41.455693
3515.338305	782903.053504	41.460698
3514.820382	782636.652406	41.465703
3515.086249	782363.127575	41.470708
3514.707454	782107.259402	41.475712
3514.888081	781844.058782	41.480717
3515.117681	781599.042062	41.485722
3514.741109	781330.995184	41.490727
3514.827207	781066.404297	41.495732
3514.437125	780820.134918	41.500736
3514.509855	780558.823952	41.505741
3514.296007	780318.117275	41.510746
3514.228580	780060.895184	41.515751
3514.325725	779811.558932	41.520756
3513.665384	779574.886746	41.525760
3513.851629	779325.371454	41.530765
3513.842947	779080.013380	41.535770
3513.871146	778839.168449	41.540775
3513.560059	778589.759011	41.545780
3513.607637	778359.377510	41.550784
3513.542796	778119.459128	41.555789
3513.272764	777879.665074	41.560794
3513.389718	777646.345641	41.565799
3513.226141	777406.518446	41.570804
3513.168819	777173.163339	41.575808
3513.354065	776947.686011	41.580813
3512.792902	776717.451271	41.585818
3512.533169	776490.457870	41.590823
3512.613335	776270.441224	41.595828
3512.213359	776041.143161	41.600832
3512.336295	775835.974146	41.605837
3512.150754	775610.171955	41.610842
3512.484258	775404.562263	41.615847
3512.040352	775179.478634	41.620852
3511.648778	774969.446389	41.625856
3512.032140	774755.538208	41.630861
3511.981229	774564.050798	41.635866
3511.676811	774343.399406	41.640871
3511.926802	774142.889270	41.645876
3511.523491	773928.446405	41.650880
3511.643693	773724.154322	41.655885
3511.453835	773518.282458	41.660890
3510.932562	773322.949551	41.665895
3510.969865	773120.870565	41.670900
3510.989172	772935.288412	41.675904
3510.982031	772730.694177	41.680909
3510.759543	772540.315073	41.685914
3510.327583	772358.191284	41.690919
3510.474167	772175.622859	41.695924
3510.416587	771987.714401	41.700928
3510.396846	771808.415331	41.705933
3510.327342	771627.149673	41.710938
3510.392914	771438.714323	41.715943
3510.538821	771253.906401	41.720948
3510.101926	771080.569957	41.725952
3509.996420	770901.952692	41.730957
3510.056841	770716.751289	41.735962
3510.109607	770557.510703	41.740967
3510.140532	770373.586528	41.745972
3509.804498	770206.075962	41.750976
3509.795052	770019.341231	41.755981
3509.635384	769856.523744	41.760986
3509.440168	769680.651023	41.765991
3509.377397	769508.447914	41.770996
3509.747262	769355.781324	41.776000
3509.660311	769183.328268	41.781005
3510.359054	769012.860700	41.786010
3509.574679	768838.839095	41.791015
3509.436192	768657.314912	41.796020
3509.101740	768505.042558	41.801024
3509.236485	768334.208811	41.806029
3509.236207	768182.219755	41.811034
3508.951983	768020.762437	41.816039
3509.039903	767847.756701	41.821044
3509.011407	767698.374553	41.826048
3508.937757	767537.759216	41.831053
3508.748126	767379.870416	41.836058
3508.743408	767221.553478	41.841063
3508.512228	767071.452799	41.846068
3508.391816	766926.851541	41.851072
3508.646992	766766.461143	41.856077
3508.528195	766620.719944	41.861082
3508.345370	766478.634270	41.866087
3508.500164	766328.997289	41.871092
3508.414159	766184.819640	41.876096
3508.298847	766034.777598	41.881101
3508.422297	765892.482408	41.886106
3508.238168	765743.234629	41.891111
3507.859481	765603.481663	41.896116
3507.975151	765460.242814	41.901120
3508.153085	765323.203084	41.906125
3507.647221	765185.188842	41.911130
3507.802681	765049.232474	41.916135
3507.726890	764901.330563	41.921140
3507.232246	764773.414456	41.926144
3507.684317	764640.458775	41.931149
3507.441360	764510.820272	41.936154
3507.103937	764381.343017	41.941159
3507.387706	764257.924863	41.946164
3507.505215	764137.687937	41.951168
3507.386093	763997.664981	41.956173
3507.373221	763868.026764	41.961178
3506.986964	763749.543237	41.966183
3506.916900	763622.671727	41.971188
3506.625396	763510.776852	41.976192
3506.872428	763387.202496	41.981197
3506.977475	763270.504436	41.986202
3506.900966	763154.376964	41.991207
3507.086316	763030.905552	41.996212
3506.700321	762913.986964	42.001216
3506.830117	762793.085357	42.006221
3506.858362	762682.753000	42.011226
3506.583169	762559.201775	42.016231
3506.640361	762442.548079	42.021236
3506.284278	762330.251704	42.026240
3506.571797	762215.184167	42.031245
3506.530591	762114.768836	42.036250
3506.510983	761999.255375	42.041255
3506.599168	761883.623731	42.046260
3506.220209	761771.717401	42.051264
3506.410677	761662.033931	42.056269
3506.679115	761553.026601	42.061274
3506.100761	761442.282764	42.066279
3506.173007	761329.259635	42.071284
3506.319730	761224.164581	42.076288
3506.217650	761111.857535	42.081293
3505.911774	761021.090631	42.086298
3506.230908	760915.568231	42.091303
3506.448339	760812.034401	42.096308
3505.645198	760701.760726	42.101312
3506.301577	760591.195615	42.106317
3506.077989	760491.627417	42.111322
3505.634571	760386.321951	42.116327
3505.755247	760278.257949	42.121332
3505.748339	760192.464060	42.126336
3505.867181	760083.262846	42.131341
3506.165687	759991.693281	42.136346
3505.573083	759882.310372	42.141351
3505.528837	759782.259246	42.146356
3505.722427	759687.101554	42.151360
3505.808346	759593.835332	42.156365
3506.052860	759496.594577	42.161370
3505.791999	759398.991778	42.166375
3506.038248	759291.287742	42.171380
3505.449653	759210.759495	42.176384
3505.600348	759103.561964	42.181389
3505.519760	759010.266660	42.186394
3505.458378	758919.532955	42.191399
3505.713947	758816.310986	42.196404
3505.457005	758741.496481	42.201408
3505.377547	758632.455091	42.206413
3505.532141	758540.891735	42.211418
3505.328657	758451.014745	42.216423
3505.491167	758360.188120	42.221428
3505.130125	758266.189667	42.226432
3505.152580	758171.485320	42.231437
3505.437265	758084.533865	42.236442
3504.784095	758005.237210	42.241447
3505.235695	757917.368035	42.246452
3505.188424	757840.832183	42.251456
3504.990881	757755.338266	42.256461
3505.096820	757666.338704	42.261466
3505.040151	757576.624599	42.266471
3505.005444	757489.867041	42.271476
3504.742905	757405.909874	42.276480
3505.057916	757319.685005	42.281485
3505.095832	757244.313636	42.286490
3504.850624	757151.072004	42.291495
3504.912433	757082.259427	42.296500
3504.792736	756999.261369	42.301504
3505.118744	756913.671738	42.306509
3504.902215	756822.346300	42.311514
3505.049341	756746.014209	42.316519
3505.113432	756657.750147	42.321524
3504.833325	756578.870750	42.326528
3504.938114	756492.917977	42.331533
3505.051113	756408.887952	42.336538
3504.728710	756336.972879	42.341543
3504.601680	756248.439410	42.346548
3504.861681	756184.522255	42.351552
3504.890713	756098.133265	42.356557
3504.732340	756009.108560	42.361562
3504.463025	755947.497990	42.366567
3504.631880	755862.070565	42.371572
3504.678790	755786.782053	42.376576
3504.495341	755707.680271	42.381581
3504.658718	755631.531832	42.386586
3504.144114	755552.828574	42.391591
3504.307401	755483.343112	42.396596
3504.412842	755417.618452	42.401600
3504.432914	755347.414848	42.406605
3504.389003	755280.479432	42.411610
3504.082589	755205.885208	42.416615
3504.526476	755124.798028	42.421620
3504.396478	755057.084941	42.426624
3504.671008	754984.861309	42.431629
3504.268593	754912.106727	42.436634
3504.320699	754842.979370	42.441639
3504.143833	754780.998574	42.446644
3503.778307	754707.841003	42.451648
3504.395735	754637.334977	42.456653
3504.640433	754566.247878	42.461658
3504.289026	754495.850821	42.466663
3504.319726	754425.538276	42.471668
3504.334366	754355.079610	42.476672
3504.206893	754275.706944	42.481677
3504.283833	754200.941020	42.486682
3504.132970	754141.666393	42.491687
3504.724650	754062.518651	42.496692
3504.174046	754001.481903	42.501696
3504.136781	753926.435867	42.506701
3504.066415	753850.950157	42.511706
3503.771301	753795.794933	42.516711
3504.365849	753724.049862	42.521716
3503.959720	753662.147182	42.526720
3503.941271	753597.760561	42.531725
3503.818031	753534.822665	42.536730
3503.847378	753476.352655	42.541735
3504.085871	753410.095079	42.546740
3504.050940	753347.832422	42.551744
3503.852453	753285.645591	42.556749
3504.039360	753209.419857	42.561754
3503.870596	753150.831872	42.566759
3504.003752	753079.996315	42.571764
3503.785919	753027.538859	42.576768
3503.696935	752953.825177	42.581773
3503.731696	752908.041363	42.586778
3503.601256	752848.506479	42.591783
3503.517468	752772.469174	42.596788
3503.575694	752726.384108	42.601792
3503.690939	752670.609964	42.606797
3503.553191	752613.988172	42.611802
3503.640555	752547.254225	42.616807
3503.846313	752496.649389	42.621812
3503.505169	752429.639330	42.626816
3503.481014	752379.120993	42.631821
3503.561263	752319.250983	42.636826
3503.006220	752270.498569	42.641831
3503.766576	752216.145846	42.646836
3503.300352	752163.377717	42.651840
3503.421474	752114.364736	42.656845
3503.780650	752056.521035	42.661850
3503.723890	752011.339639	42.666855
3503.743054	751937.944142	42.671860
3503.314667	751888.230039	42.676864
3503.381234	751827.222500	42.681869
3503.443274	751770.462811	42.686874
3503.491703	751716.372055	42.691879
3503.593960	751659.061621	42.696884
3503.232265	751601.975385	42.701888
3503.586343	751543.042065	42.706893
3503.472869	751495.990101	42.711898
3503.495426	751439.975374	42.716903
3503.525210	751384.107229	42.721908
3503.281303	751330.358298	42.726912
3503.897023	751278.097338	42.731917
3503.538674	751231.281686	42.736922
3503.074456	751171.887645	42.741927
3503.286568	751110.998651	42.746932
3503.451189	751070.171400	42.751936
3503.205172	751012.765376	42.756941
3503.808786	750958.281462	42.761946
3503.479798	750910.718092	42.766951
3503.595157	750847.916526	42.771956
3503.761678	750798.986515	42.776960
3503.479122	750741.782086	42.781965
3503.770833	750679.098283	42.786970
3503.442106	750629.507843	42.791975
3503.486955	750564.196304	42.796980
3503.610036	750505.688334	42.801985
3503.286275	750459.998477	42.806989
3503.293591	750402.595579	42.811994
3503.373332	750357.530220	42.816999
3503.545421	750294.616019	42.822004
3503.097123	750250.921446	42.827009
3503.376286	750195.497629	42.832013
3503.475475	750148.056618	42.837018
3503.369743	750099.068245	42.842023
3503.102016	750039.633127	42.847028
3503.195628	749999.009537	42.852033
3503.031976	749940.840960	42.857037
3503.119144	749889.744585	42.862042
3503.333557	749843.320177	42.867047
3503.155795	749781.398112	42.872052
3503.276019	749741.905066	42.877057
3503.433682	749688.770208	42.882061
3503.320060	749640.965931	42.887066
3503.059918	749605.289576	42.892071
3503.294597	749547.744075	42.897076
3503.396023	749493.974890	42.902081
3503.046991	749441.860530	42.907085
3503.099005	749390.173793	42.912090
3503.028575	749348.733933	42.917095
3503.157371	749297.231549	42.922100
3503.289446	749246.963450	42.927105
3503.399598	749196.945673	42.932109
3503.251330	749148.106523	42.937114
3503.101001	749101.737782	42.942119
3503.236524	749040.696927	42.947124
3503.190265	749001.474587	42.952129
3502.965783	748962.034374	42.957133
3503.345925	748910.932691	42.962138
3502.908496	748852.405795	42.967143
3503.209079	748809.567877	42.972148
3502.956117	748764.646908	42.977153
3503.146600	748717.923260	42.982157
3503.070878	748675.690121	42.987162
3503.068201	748628.207198	42.992167
3502.935177	748584.994797	42.997172
3502.871369	748542.660150	43.002177
3502.933918	748504.059715	43.007181
3503.358299	748455.121849	43.012186
3502.695595	748411.205174	43.017191
3503.321173	748350.522860	43.022196
3503.112346	748316.413319	43.027201
3502.720463	748267.213473	43.032205
3502.753652	748212.063105	43.037210
3502.893176	748179.229718	43.042215
3503.046980	748125.738920	43.047220
3503.076672	748076.863714	43.052225
3503.352781	748030.961874	43.057229
3503.180567	747986.418418	43.062234
3502.482082	747951.350252	43.067239
3503.045173	747909.946576	43.072244
3502.753249	747869.227138	43.077249
3502.858041	747833.531925	43.082253
3502.860846	747776.110358	43.087258
3502.443072	747733.829637	43.092263
3502.558358	747690.719602	43.097268
3502.389400	747663.766020	43.102273
3502.522462	747630.931388	43.107277
3502.753831	747597.981585	43.112282
3502.647881	747560.096076	43.117287
3502.934417	747516.017928	43.122292
3502.696987	747470.741003	43.127297
3502.671543	747437.190406	43.132301
3502.673355	747387.475362	43.137306
3502.634995	747347.057340	43.142311
3502.694183	747305.387561	43.147316
3502.738602	747272.714285	43.152321
3502.569220	747229.104995	43.157325
3503.143210	747190.117261	43.162330
3502.661962	747149.029895	43.167335
3502.901343	747102.634446	43.172340
3502.729615	747081.510893	43.177345
3502.892172	747029.444323	43.182349
3503.012313	746989.097171	43.187354
3502.818405	746947.071816	43.192359
3502.757453	746910.856059	43.197364
3502.773893	746866.719910	43.202369
3502.935629	746815.245109	43.207373
3503.139661	746773.449780	43.212378
3502.828548	746732.431028	43.217383
3503.067070	746689.295156	43.222388
3503.114326	746644.164215	43.227393
3502.992644	746602.372218	43.232397
3503.181278	746549.309685	43.237402
3502.912823	746506.651733	43.242407
3502.972938	746456.723460	43.247412
3502.681691	746426.078925	43.252417
3502.741393	746369.922674	43.257421
3503.052100	746323.164872	43.262426
3502.662301	746299.208473	43.267431
3502.860333	746254.099860	43.272436
3502.582603	746211.787805	43.277441
3502.505776	746173.841342	43.282445
3502.686436	746128.290032	43.287450
3502.779542	746099.854498	43.292455
3502.709952	746053.553162	43.297460
3502.460772	746010.741046	43.302465
3502.519040	745975.687562	43.307469
3502.751305	745937.787877	43.312474
3502.394903	745901.418415	43.317479
3502.563313	745863.331180	43.322484
3502.639975	745835.984815	43.327489
3502.716056	745787.977345	43.332493
3502.440112	745753.076791	43.337498
3502.435244	745716.747403	43.342503
3502.920662	745670.302919	43.347508
3502.480698	745638.147489	43.352513
3502.958018	745604.951046	43.357517
3502.794094	745559.601496	43.362522
3502.747301	745526.738233	43.367527
3502.696913	745476.475903	43.372532
3502.574831	745452.917668	43.377537
3502.813932	745415.755793	43.382541
3502.823659	745367.756680	43.387546
3502.941467	745324.089436	43.392551
3502.959571	745276.780428	43.397556
3502.767964	745244.977912	43.402561
3502.636729	745195.468580	43.407565
3502.869052	745148.667255	43.412570
3502.433760	745122.490275	43.417575
3502.763130	745080.418094	43.422580
3502.717404	745049.529974	43.427585
3502.932792	744999.665692	43.432589
3503.113967	744960.187829	43.437594
3502.798744	744921.483638	43.442599
3502.942827	744869.010272	43.447604
3503.390523	744836.309806	43.452609
3502.579872	744788.096282	43.457613
3503.034393	744742.442359	43.462618
3502.493148	744701.203695	43.467623
3502.655279	744655.004218	43.472628
3502.822674	744619.432331	43.477633
3502.929056	744590.791393	43.482637
3502.872921	744543.687940	43.487642
3502.553243	744514.672001	43.492647
3502.869731	744455.889019	43.497652
3502.363458	744432.489895	43.502657
3502.432730	744388.924319	43.507661
3502.636083	744349.785795	43.512666
3502.417616	744317.885068	43.517671
3502.796297	744271.598217	43.522676
3502.809551	744242.081467	43.527681
3502.771499	744183.898691	43.532685
3502.643897	744158.261051	43.537690
3502.701693	744118.700412	43.542695
3502.983635	744066.891119	43.547700
3502.938223	744026.061595	43.552705
3502.769999	743993.755756	43.557709
3503.138041	743950.534039	43.562714
3502.775436	743898.434322	43.567719
3502.430977	743858.988099	43.572724
3502.616281	743822.717486	43.577729
3502.192777	743790.106787	43.582733
3502.799127	743756.584635	43.587738
3502.355731	743723.433082	43.592743
3502.597853	743689.525688	43.597748
3502.733007	743656.130193	43.602753
3502.792176	743614.490229	43.607757
3502.471383	743575.088122	43.612762
3502.438255	743548.938502	43.617767
3502.448943	743500.136733	43.622772
3502.311541	743459.319425	43.627777
3502.450444	743435.909901	43.632781
3502.525529	743386.800159	43.637786
3501.956236	743368.154831	43.642791
3502.285898	743328.248757	43.647796
3502.483947	743291.924156	43.652801
3502.173844	743253.952562	43.657805
3502.422072	743235.271099	43.662810
3502.380313	743194.782772	43.667815
3502.711451	743163.083464	43.672820
3502.739298	743124.511663	43.677825
3502.629971	743090.115703	43.682829
3502.770551	743054.046703	43.687834
3502.676376	743018.560127	43.692839
3502.863836	742964.336297	43.697844
3502.896979	742937.975942	43.702849
3502.484021	742899.178994	43.707853
3502.873217	742863.068155	43.712858
3502.037279	742828.049074	43.717863
3502.638575	742784.881426	43.722868
3502.772452	742752.767947	43.727873
3502.183548	742713.900182	43.732877
3502.327818	742670.609425	43.737882
3502.465129	742656.790789	43.742887
3502.533898	742615.292307	43.747892
3502.588742	742578.246288	43.752897
3502.390996	742547.917326	43.757901
3502.675672	742513.503374	43.762906
3502.181491	742474.074876	43.767911
3502.564524	742434.897232	43.772916
3502.497647	742406.029648	43.777921
3502.419233	742363.960698	43.782925
3502.192528	742329.531309	43.787930
3502.047839	742304.978352	43.792935
3502.389764	742266.400052	43.797940
3502.267944	742243.425557	43.802945
3502.477590	742206.500638	43.807949
3502.406222	742166.160261	43.812954
3502.305078	742142.539198	43.817959
3502.247674	742108.130396	43.822964
3502.441385	742078.377996	43.827969
3502.238372	742051.460170	43.832973
3502.339575	742008.469592	43.837978
3502.250163	741987.961628	43.842983
3502.119485	741936.305232	43.847988
3502.154086	741914.589777	43.852993
3502.483901	741891.094761	43.857997
3502.638071	741848.144036	43.863002
3502.199697	741833.825382	43.868007
3502.555880	741779.516159	43.873012
3502.300158	741758.045928	43.878017
3502.332096	741720.455667	43.883021
3502.575737	741677.390364	43.888026
3502.264726	741653.851874	43.893031
3502.340066	741611.209579	43.898036
3502.358987	741574.412046	43.903041
3502.257590	741558.355893	43.908045
3502.480954	741517.617452	43.913050
3502.520244	741484.228563	43.918055
3502.674949	741446.666228	43.923060
3502.753508	741409.264630	43.928065
3502.238780	741376.164399	43.933069
3502.680897	741342.115058	43.938074
3502.250158	741304.153950	43.943079
3502.427066	741267.872981	43.948084
3502.408632	741253.731359	43.953089
3502.325692	741220.806613	43.958093
3502.140922	741186.810445	43.963098
3502.166980	741150.949458	43.968103
3502.270855	741126.104589	43.973108
3501.836311	741101.744025	43.978113
3501.887796	741071.417779	43.983117
3502.390712	741033.697191	43.988122
3501.570832	741007.322577	43.993127
3501.893035	740983.282080	43.998132
3502.113422	740961.088266	44.003137
3502.217024	740930.456140	44.008141
3502.239381	740895.633246	44.013146
3502.460636	740870.817694	44.018151
3502.502649	740846.031600	44.023156
3502.225635	740813.087677	44.028161
3502.306625	740765.147694	44.033165
3502.599784	740746.601334	44.038170
3502.364173	740712.611506	44.043175
3502.503545	740680.983313	44.048180
3502.338461	740640.007603	44.053185
3502.467211	740606.847578	44.058189
3502.436952	740563.623508	44.063194
3502.202672	740541.651823	44.068199
3502.065196	740512.047034	44.073204
3502.067611	740469.905225	44.078209
3502.151810	740454.310868	44.083213
3502.007427	740421.788619	44.088218
3501.844712	740400.398296	44.093223
3501.974606	740362.241360	44.098228
3502.218904	740356.364555	44.103233
3501.990399	740315.199764	44.108237
3502.479225	740298.499707	44.113242
3502.087773	740257.806635	44.118247
3502.278914	740229.333758	44.123252
3502.226163	740203.868783	44.128257
3502.020501	740168.239385	44.133261
3502.342550	740132.028231	44.138266
3502.171283	740110.539607	44.143271
3502.378996	740073.605065	44.148276
3502.489024	740042.374877	44.153281
3502.373986	740015.979735	44.158285
3502.493914	739970.402840	44.163290
3502.274357	739947.338849	44.168295
3502.459664	739913.671957	44.173300
3502.409075	739887.216301	44.178305
3502.214153	739848.368434	44.183309
3502.325652	739810.014011	44.188314
3502.091302	739790.760886	44.193319
3502.050697	739755.052968	44.198324
3502.091146	739722.843661	44.203329
3502.347769	739693.071941	44.208333
3502.493943	739670.392081	44.213338
3502.422832	739633.254101	44.218343
3502.561194	739603.155262	44.223348
3502.545480	739575.752943	44.228353
3502.305991	739532.953474	44.233357
3502.376765	739500.490930	44.238362
3502.232262	739465.540849	44.243367
3502.041859	739429.311999	44.248372
3502.440341	739404.907882	44.253377
3502.184634	739372.647018	44.258381
3502.069103	739343.083718	44.263386
3502.060897	739320.626174	44.268391
3502.107852	739279.212742	44.273396
3502.279435	739258.506294	44.278401
3502.163865	739229.981438	44.283405
3502.235488	739202.761320	44.288410
3502.089156	739177.110593	44.293415
3502.206680	739147.903924	44.298420
3502.293143	739113.211056	44.303425
3502.441905	739085.631534	44.308429
3502.525126	739046.387617	44.313434
3502.178741	739017.702149	44.318439
3502.248766	738984.742914	44.323444
3501.870027	738958.734007	44.328449
3502.306864	738930.067579	44.333453
3502.131416	738882.603730	44.338458
3501.817041	738873.305392	44.343463
3502.034550	738834.582494	44.348468
3501.970988	738819.949248	44.353473
3502.098913	738788.364880	44.358477
3502.549256	738767.957531	44.363482
3502.386636	738744.138573	44.368487
3502.399359	738701.392012	44.373492
3502.162598	738677.634544	44.378497
3502.141424	738640.879484	44.383501
3502.225591	738608.361620	44.388506
3502.196554	738585.806488	44.393511
3502.470089	738548.359282	44.398516
3502.325699	738516.175546	44.403521
3502.266489	738490.706144	44.408525
3502.210362	738458.606580	44.413530
3501.855028	738434.670027	44.418535
3502.472323	738401.519251	44.423540
3502.551962	738361.827278	44.428545
3502.244845	738337.288786	44.433549
3502.148361	738304.651024	44.438554
3501.866854	738267.096053	44.443559
3501.958566	738240.116713	44.448564
3502.166395	738221.281678	44.453569
3502.072635	738185.822853	44.458573
3502.302087	738160.007972	44.463578
3502.231965	738128.552576	44.468583
3502.214388	738100.056998	44.473588
3502.425681	738067.812841	44.478593
3502.310322	738041.905965	44.483597
3502.471415	738004.128393	44.488602
3502.293351	737963.239967	44.493607
3502.316015	737933.500225	44.498612
3501.982876	737916.732720	44.503617
3502.155101	737893.746643	44.508621
3502.564605	737847.417184	44.513626
3502.103023	737827.800917	44.518631
3502.482863	737799.980958	44.523636
3502.375426	737767.293321	44.528641
3502.146538	737733.240153	44.533645
3502.398742	737690.250791	44.538650
3501.878874	737658.422335	44.543655
3502.151010	737631.906002	44.548660
3502.196972	737607.010202	44.553665
3501.679677	737594.131779	44.558669
3502.169788	737558.178114	44.563674
3502.094428	737538.250092	44.568679
3502.166276	737494.695635	44.573684
3502.518813	737471.035385	44.578689
3502.321356	737444.843213	44.583693
3502.235956	737421.848748	44.588698
3502.160315	737383.414516	44.593703
3502.135320	737348.534409	44.598708
3502.128906	737325.971985	44.603713
3502.119414	737295.344498	44.608717
3502.438072	737264.266966	44.613722
3501.939124	737244.803864	44.618727
3502.271832	737211.695051	44.623732
3502.224995	737174.986946	44.628737
3501.906839	737146.290079	44.633741
3502.448294	737117.401981	44.638746
3501.979038	737094.073960	44.643751
3502.252435	737067.605032	44.648756
3502.073810	737033.441628	44.653761
3501.994454	737014.997456	44.658765
3501.884503	736975.676214	44.663770
3501.822372	736966.383560	44.668775
3502.320721	736935.572045	44.673780
3502.100090	736910.223163	44.678785
3502.214253	736889.371580	44.683789
3502.128000	736850.045814	44.688794
3501.953551	736822.610698	44.693799
3502.098660	736781.959875	44.698804
3502.281868	736772.032750	44.703809
3501.904235	736741.414316	44.708813
3502.034573	736698.340732	44.713818
3501.700627	736697.158664	44.718823
3501.663859	736657.922770	44.723828
3502.049838	736641.034083	44.728833
3501.773425	736613.714023	44.733837
3502.193797	736590.732797	44.738842
3501.964597	736561.722254	44.743847
3501.769551	736537.753587	44.748852
3502.045297	736514.251624	44.753857
3501.948414	736494.621464	44.758861
3502.316948	736454.229080	44.763866
3502.229823	736439.397401	44.768871
3501.965345	736395.298530	44.773876
3501.702320	736374.458270	44.778881
3501.845053	736350.136458	44.783885
3501.926367	736327.160860	44.788890
3501.897172	736316.921759	44.793895
3501.845661	736271.302480	44.798900
3502.036319	736258.899093	44.803905
3501.820375	736238.199184	44.808909
3502.106968	736219.148506	44.813914
3501.942164	736191.462193	44.818919
3502.328586	736163.783931	44.823924
3502.320006	736129.489667	44.828929
3502.265500	736108.317421	44.833933
3501.994612	736078.173745	44.838938
3501.885303	736053.546140	44.843943
3501.778011	736018.030430	44.848948
3502.005502	735991.268574	44.853953
3502.062935	735971.512723	44.858957
3502.190396	735940.956462	44.863962
3502.408870	735917.412698	44.868967
3502.187597	735878.351856	44.873972
3501.817301	735855.548302	44.878977
3501.935900	735830.585513	44.883981
3502.088666	735798.242873	44.888986
3502.046032	735782.907737	44.893991
3501.913315	735743.485208	44.898996
3502.231275	735717.053969	44.904001
3502.298201	735696.949438	44.909005
3502.644551	735660.466545	44.914010
3502.058599	735629.878179	44.919015
3502.083452	735594.536784	44.924020
3502.004496	735579.405213	44.929025
3501.934651	735543.287320	44.934029
3502.514788	735512.902301	44.939034
3502.007927	735492.050428	44.944039
3501.993770	735453.151356	44.949044
3502.524285	735425.496301	44.954049
3502.074466	735397.854208	44.959053
3502.624510	735374.551177	44.964058
3502.069234	735345.787930	44.969063
3502.347546	735301.098656	44.974068
3502.349988	735278.825967	44.979073
3502.146115	735249.954978	44.984077
3502.139393	735225.901856	44.989082
3502.115071	735200.119252	44.994087
3502.180289	735165.957190	44.999092
3502.225607	735135.510388	45.004097
3501.991908	735105.158942	45.009101
3502.457432	735069.247670	45.014106
3502.129975	735049.750952	45.019111
3502.355732	735009.622305	45.024116
3501.951338	734994.097792	45.029121
3502.140068	734953.282022	45.034125
3501.944329	734927.427795	45.039130
3501.866865	734907.097597	45.044135
3502.006489	734867.576390	45.049140
3501.907549	734854.327616	45.054145
3502.023720	734821.294117	45.059149
3501.898946	734801.169433	45.064154
3501.654574	734782.747311	45.069159
3501.919090	734752.757911	45.074164
3501.977763	734737.651570	45.079169
3501.743839	734704.378294	45.084173
3502.250274	734681.872410	45.089178
3501.654239	734655.142807	45.094183
3501.717802	734638.501037	45.099188
3501.934588	734602.826663	45.104193
3501.529436	734591.063362	45.109197
3502.036602	734567.121583	45.114202
3501.437806	734551.430250	45.119207
3501.523150	734530.181295	45.124212
3501.651160	734513.479148	45.129217
3501.234119	734493.946341	45.134221
3501.649085	734482.740728	45.139226
3501.450036	734469.408816	45.144231
3501.686852	734431.453422	45.149236
3501.845456	734430.734336	45.154241
3501.784713	734408.568644	45.159245
3502.005053	734378.931627	45.164250
3501.781951	734361.247527	45.169255
3501.606334	734335.586078	45.174260
3501.513061	734322.236492	45.179265
3501.419592	734302.006399	45.184269
3501.882562	734267.675978	45.189274
3501.999402	734261.370216	45.194279
3501.918579	734229.158753	45.199284
3501.555301	734215.308973	45.204289
3502.169800	734187.685333	45.209293
3502.360663	734161.913440	45.214298
3501.660519	734134.308237	45.219303
3502.033068	734109.694268	45.224308
3501.910731	734079.023584	45.229313
3501.942709	734057.039651	45.234317
3502.064653	734022.764381	45.239322
3502.029799	734004.454454	45.244327
3502.092777	733976.623958	45.249332
3502.284117	733952.088870	45.254337
3502.070957	733925.541256	45.259341
3502.517747	733888.637760	45.264346
3502.027163	733864.016759	45.269351
3502.045545	733830.648788	45.274356
3501.984678	733809.323017	45.279361
3501.936435	733782.252724	45.284365
3502.059284	733752.480958	45.289370
3501.804714	733729.602781	45.294375
3501.775413	733706.142877	45.299380
3502.056041	733688.621812	45.304385
3501.871257	733657.266756	45.309389
3501.759433	733625.355009	45.314394
3501.969418	733616.954215	45.319399
3501.817799	733584.306296	45.324404
3501.971410	733563.736607	45.329409
3501.947001	733537.107105	45.334413
3501.915924	733515.033073	45.339418
3501.841436	733490.193847	45.344423
3501.755361	733473.772348	45.349428
3501.855543	733430.042638	45.354433
3501.693604	733413.683022	45.359437
3501.809120	733396.980621	45.364442
3501.443618	733382.585207	45.369447
3501.926350	733357.802273	45.374452
3501.791079	733333.022084	45.379457
3501.755047	733302.136195	45.384461
3502.217610	733292.901345	45.389466
3502.041983	733265.949320	45.394471
3501.811122	733237.174559	45.399476
3502.121810	733214.251281	45.404481
3501.881714	733191.963273	45.409485
3502.168795	733143.448543	45.414490
3501.889239	733134.929885	45.419495
3502.021463	733099.114268	45.424500
3502.256051	733077.589354	45.429505
3501.892108	733056.262022	45.434509
3502.504126	733021.951253	45.439514
3502.108796	733000.529930	45.444519
3502.076790	732957.017471	45.449524
3502.205730	732945.757847	45.454529
3501.892283	732908.628585	45.459533
3502.328793	732888.604664	45.464538
3502.066829	732865.180651	45.469543
3502.071091	732850.921392	45.474548
3502.392476	732814.726781	45.479553
3502.052822	732780.423275	45.484557
3501.941538	732754.548147	45.489562
3501.782425	732724.769541	45.494567
3501.993878	732692.602793	45.499572
3502.233296	732680.730475	45.504577
3501.930961	732651.569320	45.509581
3502.198250	732628.800065	45.514586
3501.754862	732605.454703	45.519591
3502.106066	732571.729618	45.524596
3502.097154	732550.342446	45.529601
3501.931673	732516.504226	45.534605
3502.298642	732483.370309	45.539610
3502.182624	732466.951693	45.544615
3502.185993	732435.115277	45.549620
3501.936328	732397.626571	45.554625
3502.116241	732378.980492	45.559629
3502.474306	732354.116005	45.564634
3502.216833	732325.193838	45.569639
3502.145136	732291.883859	45.574644
3502.216941	732266.670173	45.579649
3501.924773	732243.645432	45.584653
3502.006089	732204.021752	45.589658
3501.990467	732173.870879	45.594663
3501.966999	732157.238330	45.599668
3501.993043	732131.190036	45.604673
3501.897700	732106.944149	45.609677
3502.334647	732073.202860	45.614682
3502.085274	732054.527744	45.619687
3502.085834	732018.134865	45.624692
3502.232972	731996.274885	45.629697
3501.744433	731971.499211	45.634701
3502.160481	731946.574405	45.639706
3502.163171	731916.419554	45.644711
3501.791318	731888.802056	45.649716
3502.043139	731870.539077	45.654721
3501.820036	731852.205770	45.659725
3502.217613	731815.449468	45.664730
3501.909348	731800.497123	45.669735
3501.560681	731769.409310	45.674740
3501.985673	731743.987251	45.679745
3501.646526	731726.217453	45.684749
3501.898097	731700.823834	45.689754
3501.727824	731678.817235	45.694759
3501.953700	731646.990568	45.699764
3501.479853	731642.711240	45.704769
3502.033624	731612.117834	45.709773
3501.742614	731588.645385	45.714778
3501.884131	731566.488071	45.719783
3501.824612	731539.857769	45.724788
3501.800066	731512.132237	45.729793
3501.842538	731490.238621	45.734797
3501.690090	731480.063191	45.739802
3502.086298	731456.477120	45.744807
3501.555889	731432.152348	45.749812
3501.739640	731414.543290	45.754817
3501.648009	731373.904169	45.759821
3501.947111	731285.959817	45.764826
3501.676512	731159.433819	45.769831
3501.482486	730974.657281	45.774836
3501.365325	730721.721765	45.779841
3501.155486	730419.913666	45.784845
3500.928321	730068.967494	45.789850
3500.940326	729652.638790	45.794855
3500.768524	729187.134502	45.799860
3500.498563	728636.024119	45.804865
3499.991649	728063.069186	45.809869
3499.607963	727420.249130	45.814874
3498.938743	726726.392997	45.819879
3498.674895	725953.575973	45.824884
3498.176301	725145.788017	45.829889
3497.686591	724268.087818	45.834893
3497.041644	723329.600567	45.839898
3496.587887	722356.323940	45.844903
3496.084592	721298.855518	45.849908
3495.580155	720189.931612	45.854913
3494.581153	719020.041993	45.859917
3493.872400	717776.235351	45.864922
3493.319680	716498.038685	45.869927
3492.113768	715150.244144	45.874932
3491.185891	713748.346621	45.879937
3490.535588	712278.671229	45.884941
3489.761950	710754.404671	45.889946
3488.468739	709174.491641	45.894951
3487.780976	707547.904072	45.899956
3486.708231	705831.120391	45.904961
3485.489531	704084.906626	45.909965
3484.115317	702277.744654	45.914970
3482.764021	700426.119104	45.919975
3481.662741	698511.920898	45.924980
3480.395147	696535.527832	45.929985
3478.842971	694513.978607	45.934989
3477.610384	692449.085248	45.939994
3475.900505	690327.915152	45.944999
3474.838041	688147.956354	45.950004
3473.641912	685924.879659	45.955009
3471.667529	683639.890800	45.960013
3470.364524	681321.446243	45.965018
3468.787378	678947.958848	45.970023
3467.103689	676519.013542	45.975028
3465.492230	674045.308196	45.980033
3463.745620	671529.488391	45.985037
3461.920696	668961.790402	45.990042
3460.177224	666351.678906	45.995047
3458.299548	663709.788522	46.000052
3456.574110	660999.464130	46.005057
3454.385564	658257.252962	46.010061
3452.857380	655466.168201	46.015066
3450.935327	652635.840035	46.020071
3448.647033	649757.391797	46.025076
3446.782944	646842.404986	46.030081
3444.285983	643889.929173	46.035085
3442.766551	640889.070300	46.040090
3440.411814	637863.906502	46.045095
3437.976734	634787.425876	46.050100
3435.835440	631667.138490	46.055105
3433.646410	628524.401859	46.060109
3431.607373	625338.485356	46.065114
3428.933427	622115.401152	46.070119
3426.538359	618850.213333	46.075124
3424.336104	615550.678846	46.080129
3421.779990	612222.283095	46.085133
3419.575240	608845.631037	46.090138
3416.667645	605444.548384	46.095143
3414.240414	601997.044548	46.100148
3411.675374	598530.253987	46.105153
3408.921787	595029.764794	46.110157
3406.694631	591498.103436	46.115162
3403.895905	587944.430780	46.120167
3401.244180	584347.558134	46.125172
3398.557668	580732.833117	46.130177
3395.364998	577079.909082	46.135181
3392.467687	573391.803185	46.140186
3389.822631	569700.212307	46.145191
3386.826635	565963.512058	46.150196
3384.278951	562212.163052	46.155201
3380.814106	558438.131018	46.160205
3378.179726	554630.793617	46.165210
3375.072804	550804.565165	46.170215
3372.477226	546952.224417	46.175220
3369.317985	543074.042860	46.180225
3366.174213	539173.651764	46.185229
3363.498929	535239.015707	46.190234
3360.436866	531292.218352	46.195239
3356.895699	527311.219875	46.200244
3354.078267	523314.646545	46.205249
3350.629093	519310.504946	46.210253
3347.773675	515269.148667	46.215258
3344.585724	511225.285855	46.220263
3341.339019	507149.972464	46.225268
3338.185309	503054.755956	46.230273
3334.755071	498947.033542	46.235277
3331.575297	494815.597934	46.240282
3327.684234	490673.056073	46.245287
3324.547754	486518.619947	46.250292
3321.238160	482341.821807	46.255297
3317.591193	478155.198657	46.260301
3314.530310	473941.289337	46.265306
3310.774438	469738.653605	46.270311
3307.406308	465503.311108	46.275316
3303.847212	461270.121483	46.280321
3300.411931	457016.749914	46.285325
3296.860701	452753.687184	46.290330
3293.476135	448487.594296	46.295335
3289.601479	444194.200601	46.300340
3286.505101	439905.717894	46.305345
3282.667784	435596.135912	46.310349
3279.286833	431273.994438	46.315354
3275.695151	426964.492004	46.320359
3272.266215	422625.126396	46.325364
3268.244750	418285.198295	46.330369
3264.291913	413927.783463	46.335373
3260.825141	409578.653807	46.340378
3256.768077	405220.459379	46.345383
3253.499842	400862.744698	46.350388
3249.646771	396485.785851	46.355393
3245.340087	392120.551341	46.360397
3241.912423	387743.744027	46.365402
3238.129875	383371.674012	46.370407
3234.149716	378994.473966	46.375412
3230.368490	374616.699460	46.380417
3226.471104	370232.320029	46.385421
3222.712825	365850.416825	46.390426
3218.648396	361470.169319	46.395431
3215.043307	357083.078117	46.400436
3211.439615	352696.309883	46.405441
3207.215901	348306.069783	46.410445
3203.170481	343923.696499	46.415450
3199.167780	339532.134448	46.420455
3195.211166	335143.032101	46.425460
3191.640824	330757.245628	46.430465
3187.157979	326379.796071	46.435469
3183.639627	321995.326635	46.440474
3179.547829	317627.658222	46.445479
3175.208037	313256.393781	46.450484
3171.638831	308889.965326	46.455489
3167.500038	304539.792756	46.460493
3163.354232	300171.507516	46.465498
3159.129401	295836.474636	46.470503
3155.145773	291497.970565	46.475508
3150.918637	287164.753177	46.480513
3147.053904	282837.634312	46.485517
3142.813146	278515.406321	46.490522
3138.695740	274213.873205	46.495527
3134.844333	269911.231582	46.500532
3130.487242	265619.878298	46.505537
3126.397314	261337.031393	46.510541
3122.465983	257057.532581	46.515546
3118.042922	252791.033372	46.520551
3114.093030	248537.138811	46.525556
3109.946330	244291.877600	46.530561
3105.703719	240059.147971	46.535565
3101.829357	235843.271562	46.540570
3097.507751	231624.001808	46.545575
3093.377725	227424.883783	46.550580
3089.289985	223227.420326	46.555585
3085.073207	219043.599977	46.560589
3081.360443	214867.682060	46.565594
3077.113417	210615.985507	46.570599
3072.682830	206466.433727	46.575604
3068.297476	202336.034485	46.580609
3063.816460	198218.830040	46.585613
3059.739315	194099.263204	46.590618
3055.663368	190009.935080	46.595623
3051.353646	185926.079574	46.600628
3047.156662	181852.019808	46.605633
3043.146166	177810.546773	46.610637
3038.926214	173767.789488	46.615642
3034.699097	169751.859288	46.620647
3030.207050	165743.345018	46.625652
3026.136953	161744.220598	46.630657
3021.558116	157778.779413	46.635661
3017.378876	153818.213046	46.640666
3013.025554	149881.805404	46.645671
3008.892325	145952.817783	46.650676
3004.368407	142050.471263	46.655681
3000.195566	138164.848851	46.660685
2995.691377	134292.996139	46.665690
2991.267044	130457.616078	46.670695
2987.054873	126625.369941	46.675700
2982.975883	122801.708843	46.680705
2978.271433	119022.999964	46.685709
2974.043475	115248.080559	46.690714
2969.539807	111507.974192	46.695719
2965.284916	107763.379763	46.700724
2961.252894	104059.682803	46.705729
2956.169702	100371.527386	46.710733
2952.246084	96700.617567	46.715738
2947.616939	93061.397849	46.720743
2942.973829	89440.802671	46.725748
2938.571250	85838.857123	46.730753
2933.500799	82265.774126	46.735757
2929.415637	78717.315583	46.740762
2925.162905	75209.910381	46.745767
2920.132298	71724.574141	46.750772
2915.629577	68250.226952	46.755777
2910.990340	64815.072867	46.760781
2906.168039	61411.088402	46.765786
2901.421584	58037.370231	46.770791
2896.109978	54705.180532	46.775796
2891.095876	51396.935681	46.780801
2885.893770	48150.790467	46.785805
2880.027295	44942.295064	46.790810
2873.600197	41801.339401	46.795815
2864.622268	38785.614364	46.800820
2853.910892	35893.621188	46.805825
2843.271446	33108.083780	46.810829
2833.593780	30452.510388	46.815834
2823.700983	27942.381206	46.820839
2814.293944	25561.018144	46.825844
2805.592360	23314.604043	46.830849
2796.307509	21209.169408	46.835853
2788.331508	19220.117178	46.840858
2780.294214	17374.897897	46.845863
2773.034807	15645.029764	46.850868
2765.790928	14039.051035	46.855873
2758.394387	12537.214536	46.860877
2751.326000	11152.293403	46.865882
2743.796517	9882.651091	46.870887
2735.812982	8733.825528	46.875892
2728.506809	7678.836497	46.880897
2720.491156	6749.922031	46.885901
2713.619132	5917.517037	46.890906
2706.289468	5185.238423	46.895911
2699.711318	4544.466248	46.900916
2693.899829	3981.596384	46.905921
2688.190025	3496.132981	46.910925
2683.597760	3056.534984	46.915930
2678.846739	2685.271879	46.920935
2674.640650	2354.312945	46.925940
2671.183022	2070.818323	46.930945
2667.234876	1807.634116	46.935949
2664.159988	1574.086749	46.940954
2661.056565	1362.056900	46.945959
2658.010253	1158.964527	46.950964
2654.752368	976.832764	46.955969
2651.296149	802.182989	46.960973
2648.537085	623.360344	46.965978
2644.907757	478.122446	46.970983
2640.968559	352.354717	46.975988
2637.410437	233.567620	46.980993
2630.822499	208.195675	46.985997
2624.008848	225.929737	46.991002
2619.590563	221.961059	46.996007
2616.420874	227.293789	47.001012
2614.427937	217.490094	47.006017
2612.013835	224.331512	47.011021
2609.708294	215.485402	47.016026
2607.072109	212.064677	47.021031
2604.084184	216.884127	47.026036
2601.015250	214.404899	47.031041
2597.696712	212.900681	47.036045
2594.325216	216.220308	47.041050
2591.497544	222.142302	47.046055
2588.387502	218.177973	47.051060
2585.146442	212.869676	47.056065
2581.327698	212.735867	47.061069
2578.354444	205.177115	47.066074
2574.632142	220.812833	47.071079
2571.232345	221.787218	47.076084
2568.195498	207.302656	47.081089
2565.046681	221.520169	47.086093
2562.129949	217.973494	47.091098
2558.528681	221.046108	47.096103
2554.909727	222.914317	47.101108
2551.636019	213.192590	47.106113
2547.821730	214.218431	47.111117
2544.427181	213.559965	47.116122
2541.275311	213.889787	47.121127
2537.579223	220.310154	47.126132
2534.651828	201.330107	47.131137
2531.040933	211.847203	47.136141
2528.134699	212.951703	47.141146
2524.927188	212.559179	47.146151
2521.355034	205.313233	47.151156
2518.152243	203.855089	47.156161
2514.210469	210.952442	47.161165
2510.750822	208.784042	47.166170
2507.137132	205.118199	47.171175
2503.163189	207.374595	47.176180
2500.508686	203.193843	47.181185
2496.480407	207.908792	47.186189
2492.943206	199.207838	47.191194
2490.268437	195.669031	47.196199
2486.617033	206.424712	47.201204
2483.397988	194.701880	47.206209
2479.953054	206.320788	47.211213
2476.704269	199.997942	47.216218
2473.523380	209.011801	47.221223
2469.674862	206.004594	47.226228
2466.214077	198.947913	47.231233
2462.736183	204.392774	47.236237
2458.540699	196.196374	47.241242
2455.393628	196.126043	47.246247
2452.336765	196.996736	47.251252
2449.196052	200.322168	47.256257
2444.860006	202.293233	47.261261
2441.877097	195.389565	47.266266
2438.674033	200.686852	47.271271
2435.147441	208.887134	47.276276
2431.606438	196.933910	47.281281
2427.124083	201.199929	47.286285
2423.995165	195.953164	47.291290
2421.200408	193.670537	47.296295
2417.899271	199.898892	47.301300
2414.658824	191.474827	47.306305
2410.762721	195.864906	47.311309
2407.078962	196.388982	47.316314
2403.711893	196.708041	47.321319
2400.253738	203.212554	47.326324
2396.491931	200.343439	47.331329
2393.102885	206.328992	47.336333
2389.825105	194.669013	47.341338
2386.560661	202.948004	47.346343
2382.652761	202.143508	47.351348
2379.410389	197.803136	47.356353
2375.962954	202.903995	47.361357
2372.196317	192.313406	47.366362
2368.884400	197.976021	47.371367
2365.592848	197.872962	47.376372
2362.163729	183.617921	47.381377
2358.554024	198.395081	47.386381
2355.136663	195.405593	47.391386
2351.281138	191.728687	47.396391
2348.044948	193.894587	47.401396
2344.672397	186.975787	47.406401
2340.768529	192.673586	47.411405
2337.799828	183.665984	47.416410
2333.972922	193.474093	47.421415
2330.397635	195.150540	47.426420
2327.397852	190.367782	47.431425
2323.434084	192.031408	47.436429
2320.081747	190.794241	47.441434
2316.651632	187.527061	47.446439
2312.996897	201.443392	47.451444
2309.929827	195.087512	47.456449
2306.014120	186.859870	47.461453
2302.904234	185.937702	47.466458
2299.404666	188.809781	47.471463
2295.775941	189.951208	47.476468
2292.306998	186.419707	47.481473
2288.746041	186.316186	47.486477
2284.865853	191.632212	47.491482
2281.461950	179.919151	47.496487
2277.883986	189.803217	47.501492
2275.019172	183.749450	47.506497
2271.538058	192.732860	47.511501
2268.171324	186.981801	47.516506
2264.388000	178.285766	47.521511
2260.779537	184.978574	47.526516
2257.651180	170.730021	47.531521
2254.006159	180.691080	47.536525
2250.976448	176.658471	47.541530
2247.103092	183.931392	47.546535
2242.835278	180.947822	47.551540
2239.896353	180.779719	47.556545
2236.096699	187.670075	47.561549
2232.795071	179.455963	47.566554
2229.532888	179.485298	47.571559
2226.308806	171.516314	47.576564
2222.686563	174.937961	47.581569
2218.850564	176.629512	47.586573
2215.250964	178.466348	47.591578
2211.600854	176.979260	47.596583
2208.114487	168.025858	47.601588
2205.073717	178.931096	47.606593
2201.382238	178.582981	47.611597
2198.388196	166.349233	47.616602
2194.532736	178.682752	47.621607
2190.984415	172.614424	47.626612
2187.716430	173.855419	47.631617
2183.703621	174.095361	47.636621
2180.110962	175.662300	47.641626
2176.925322	181.680897	47.646631
2173.217670	178.433013	47.651636
2170.420257	175.840563	47.656641
2166.743994	175.587249	47.661645
2162.947972	176.046768	47.666650
2159.641243	174.785609	47.671655
2155.702025	174.767538	47.676660
2152.658444	175.268383	47.681665
2148.899249	173.667732	47.686669
2145.482226	174.499812	47.691674
2142.117984	177.124488	47.696679
2138.735815	173.948984	47.701684
2135.396005	169.600809	47.706689
2131.566892	187.350130	47.711693
2127.891363	176.363663	47.716698
2124.595264	179.337833	47.721703
2120.923336	177.045724	47.726708
2117.603987	173.194041	47.731713
2114.065550	180.481804	47.736717
2110.661824	168.868323	47.741722
2107.204185	179.605844	47.746727
2103.374657	169.774993	47.751732
2099.944518	165.736389	47.756737
2096.460171	172.138058	47.761741
2093.165586	168.919117	47.766746
2089.522358	164.423549	47.771751
2086.187324	169.436364	47.776756
2082.814437	160.775728	47.781761
2079.034731	169.961296	47.786765
2075.739239	165.740235	47.791770
2071.756753	166.225488	47.796775
2068.378090	164.353472	47.801780
2065.188953	158.280991	47.806785
2061.713903	168.997332	47.811789
2058.288079	168.740434	47.816794
2054.590743	165.479696	47.821799
2050.936036	166.181385	47.826804
2047.743731	164.134550	47.831809
2043.861700	166.762316	47.836813
2040.560401	161.044442	47.841818
2037.133451	159.252848	47.846823
2033.640273	169.680337	47.851828
2030.196348	163.696727	47.856833
2026.600016	167.303876	47.861837
2022.962807	161.717468	47.866842
2020.098083	165.640108	47.871847
2016.041891	166.752880	47.876852
2012.732303	164.879758	47.881857
2008.743799	171.333570	47.886861
2005.309313	169.359126	47.891866
2002.353889	170.007520	47.896871
1998.773203	174.746210	47.901876
1995.542107	160.477943	47.906881
1991.730930	164.150398	47.911885
1988.040953	165.036156	47.916890
1984.595988	164.524551	47.921895
1980.712191	170.106615	47.926900
1977.457899	160.154433	47.931905
1973.921568	165.361003	47.936909
1970.898723	159.094768	47.941914
1967.499999	159.030206	47.946919
1963.508591	175.395058	47.951924
1960.304062	159.730605	47.956929
1956.560077	173.896307	47.961933
1952.938779	165.894470	47.966938
1949.822414	161.619447	47.971943
1946.025006	170.885782	47.976948
1942.539833	154.769423	47.981953
1939.169575	170.576629	47.986957
1935.718749	160.881710	47.991962
1932.029996	156.661578	47.996967
1928.649428	163.673156	48.001972
1925.174039	160.913216	48.006977
1921.654322	173.101864	48.011981
1917.902888	161.076121	48.016986
1914.670062	163.226350	48.021991
1911.176258	172.286466	48.026996
1907.972502	165.717246	48.032001
1904.148706	167.651133	48.037005
1900.670994	160.643299	48.042010
1896.901943	173.342220	48.047015
1893.132063	166.169525	48.052020
1890.300148	165.884897	48.057025
1886.476461	168.049666	48.062029
1882.900941	161.498856	48.067034
1879.676999	170.446728	48.072039
1875.694935	174.499750	48.077044
1872.789772	176.428145	48.082049
1869.277791	173.080300	48.087053
1865.917338	169.325185	48.092058
1862.129697	171.025405	48.097063
1858.675756	169.073819	48.102068
1855.446257	166.610958	48.107073
1851.664059	164.890220	48.112077
1848.003193	172.502478	48.117082
1844.716055	167.043686	48.122087
1840.903042	170.741426	48.127092
1837.573162	165.547227	48.132097
1834.196703	164.699202	48.137101
1830.732748	167.262609	48.142106
1827.092773	159.810003	48.147111
1823.452288	179.358849	48.152116
1820.172574	170.340446	48.157121
1816.534413	172.941918	48.162125
1813.342090	159.488719	48.167130
1809.643885	157.737171	48.172135
1805.682646	170.784035	48.177140
1803.094609	158.235270	48.182145
1798.992085	165.645630	48.187149
1795.535413	161.854762	48.192154
1792.365352	169.900632	48.197159
1788.413471	167.278517	48.202164
1785.243941	167.385202	48.207169
1781.476324	170.680219	48.212173
1777.785650	168.375694	48.217178
1774.679370	172.924473	48.222183
1771.314803	166.244969	48.227188
1767.322842	160.074848	48.232193
1763.669804	164.452882	48.237197
1760.571298	162.465147	48.242202
1757.275061	158.544005	48.247207
1753.702301	154.399383	48.252212
1750.264862	164.061441	48.257217
1746.480258	174.752555	48.262221
1742.995264	162.159218	48.267226
1739.721331	164.822525	48.272231
1735.929665	165.539384	48.277236
1733.156984	161.117351	48.282241
1728.832929	159.703310	48.287245
1725.443940	157.948695	48.292250
1722.310773	160.520082	48.297255
1718.156191	159.249933	48.302260
1715.035124	152.143269	48.307265
1711.318752	162.679070	48.312269
1707.982540	145.309700	48.317274
1704.550061	147.715649	48.322279
1700.783949	151.015804	48.327284
1697.589584	151.214467	48.332289
1694.394435	154.138888	48.337293
1690.466514	154.695562	48.342298
1687.350603	158.637787	48.347303
1683.410978	154.949302	48.352308
1680.097536	149.931301	48.357313
1676.600326	160.682912	48.362317
1672.824670	155.882578	48.367322
1669.299454	155.632913	48.372327
1665.662129	158.448468	48.377332
1662.721763	155.485872	48.382337
1658.956298	153.920203	48.387341
1655.964993	154.549085	48.392346
1652.303464	149.587239	48.397351
1648.533408	159.054094	48.402356
1645.110374	154.612493	48.407361
1641.070118	155.356296	48.412365
1637.904354	149.597788	48.417370
1634.480751	157.929351	48.422375
1630.639272	154.115962	48.427380
1627.601446	153.163588	48.432385
1624.176955	158.944325	48.437389
1620.748081	158.449668	48.442394
1617.109145	155.913734	48.447399
1613.406478	165.397109	48.452404
1610.071075	152.198414	48.457409
1606.395827	162.097787	48.462413
1602.814235	151.196532	48.467418
1599.533745	157.551619	48.472423
1595.890796	149.132359	48.477428
1592.436476	142.961971	48.482433
1588.834077	151.195823	48.487437
1585.679857	147.260027	48.492442
1582.048848	149.655062	48.497447
1578.599145	147.363768	48.502452
1575.129005	142.380427	48.507457
1571.261334	149.223090	48.512461
1567.786298	148.286173	48.517466
1564.282489	153.139940	48.522471
1560.742145	158.710756	48.527476
1557.494205	152.348220	48.532481
1553.684318	155.347482	48.537485
1550.332309	153.396851	48.542490
1547.025431	157.956419	48.547495
1543.159306	150.840793	48.552500
1540.014323	142.537224	48.557505
1536.281755	147.395661	48.562509
1533.033875	148.214630	48.567514
1529.786023	144.650740	48.572519
1525.745315	153.123623	48.577524
1522.497513	142.996692	48.582529
1518.962403	154.444356	48.587533
1515.274732	144.489186	48.592538
1511.917155	148.915268	48.597543
1508.417792	149.682080	48.602548
1505.066484	149.070892	48.607553
1501.044995	150.847734	48.612557
1497.813395	146.805993	48.617562
1494.497286	143.173094	48.622567
1491.073544	145.920328	48.627572
1487.529184	144.210119	48.632577
1483.540866	151.883845	48.637581
1480.381397	146.774048	48.642586
1476.916809	144.415436	48.647591
1473.127494	145.477656	48.652596
1469.861948	144.350886	48.657601
1466.357418	142.107025	48.662605
1463.061290	149.337601	48.667610
1459.619419	147.365975	48.672615
1455.366978	151.012116	48.677620
1452.465791	147.417233	48.682625
1448.433267	148.771866	48.687629
1445.152833	150.112116	48.692634
1441.994627	151.034335	48.697639
1438.672261	144.916658	48.702644
1435.386375	149.233064	48.707649
1431.361727	149.298195	48.712653
1427.605926	149.659497	48.717658
1424.310964	144.849001	48.722663
1420.774635	147.775131	48.727668
1417.342980	140.167291	48.732673
1413.567376	146.022380	48.737677
1410.265413	140.780688	48.742682
1406.664382	144.442538	48.747687
1402.921759	148.720792	48.752692
1399.968502	145.859764	48.757697
1397.065617	150.459414	48.762701
1393.558008	141.190928	48.767706
1389.379630	140.263445	48.772711
1385.440672	156.929227	48.777716
1382.231284	139.690356	48.782721
1378.487561	150.190246	48.787725
1375.479463	137.838904	48.792730
1371.867529	140.166217	48.797735
1367.691644	142.103079	48.802740
1364.758257	145.344192	48.807745
1361.349026	156.809435	48.812749
1358.003875	140.001316	48.817754
1354.301884	140.583483	48.822759
1350.226352	143.658784	48.827764
1347.471736	144.260777	48.832769
1343.679246	152.743488	48.837773
1340.611801	147.599245	48.842778
1336.996853	136.408339	48.847783
1332.844389	139.816056	48.852788
1329.556936	143.408368	48.857793
1325.908846	142.140695	48.862797
1322.444268	142.359024	48.867802
1319.751982	145.795140	48.872807
1316.041718	145.629616	48.877812
1312.762811	134.408048	48.882817
1308.195699	143.124406	48.887821
1304.888664	140.548468	48.892826
1301.771998	142.934862	48.897831
1297.991257	146.185256	48.902836
1295.471884	144.157757	48.907841
1291.420953	141.270662	48.912845
1287.990266	141.586622	48.917850
1284.441596	144.124956	48.922855
1280.659298	142.327358	48.927860
1276.834817	137.081177	48.932865
1273.710282	150.199460	48.937869
1269.821883	144.782497	48.942874
1266.777352	137.969396	48.947879
1262.984792	149.715531	48.952884
1259.783377	144.005629	48.957889
1256.121607	149.542661	48.962893
1252.951480	146.397110	48.967898
1249.142470	144.344852	48.972903
1245.873949	147.320968	48.977908
1242.461472	143.249134	48.982913
1238.597990	141.805201	48.987917
1235.094137	142.982435	48.992922
1231.486265	133.805855	48.997927
1227.800238	137.090966	49.002932
1224.640488	135.390790	49.007937
1221.243242	143.032909	49.012941
1217.715519	136.350841	49.017946
1214.229897	135.534544	49.022951
1210.754967	145.639643	49.027956
1207.336045	134.504460	49.032961
1203.535748	136.409960	49.037965
1200.004119	132.076659	49.042970
1196.676307	140.549939	49.047975
1193.123369	143.064380	49.052980
1189.714870	134.741309	49.057985
1186.169724	134.985297	49.062989
1182.698479	130.689387	49.067994
1179.282180	138.105180	49.072999
1175.251748	136.862167	49.078004
1172.001646	137.541056	49.083009
1168.450345	138.241527	49.088013
1165.435018	136.113174	49.093018
1161.686386	138.423388	49.098023
1157.730143	132.367132	49.103028
1154.490997	127.299176	49.108033
1150.888989	137.522212	49.113037
1147.497584	134.187378	49.118042
1144.374854	139.243257	49.123047
1140.599281	137.556952	49.128052
1137.279515	132.228039	49.133057
1133.447492	137.939931	49.138061
1130.140007	130.843625	49.143066
1126.755716	141.923627	49.148071
1123.047661	143.220946	49.153076
1119.363031	133.815619	49.158081
1116.042268	141.127844	49.163085
1112.355350	139.266864	49.168090
1109.154696	129.449604	49.173095
1105.286739	133.314670	49.178100
1101.993560	126.713508	49.183105
1098.564833	138.519373	49.188109
1095.224110	136.167024	49.193114
1091.729648	129.572117	49.198119
1087.895119	138.082288	49.203124
1084.635978	128.528494	49.208129
1080.711182	133.193506	49.213133
1077.498543	136.860447	49.218138
1074.268611	149.223696	49.223143
1070.280260	146.490244	49.228148
1067.251214	135.867528	49.233153
1063.309975	135.904194	49.238157
1059.835775	141.019431	49.243162
1056.735275	137.709578	49.248167
1052.797199	142.145534	49.253172
1049.651888	132.854147	49.258177
1046.332255	150.475462	49.263181
1042.340907	138.941345	49.268186
1038.998803	133.625676	49.273191
1035.462650	142.245601	49.278196
1032.030042	137.703265	49.283201
1028.430751	145.168566	49.288205
1024.907501	144.358245	49.293210
1021.575081	138.041480	49.298215
1017.708914	150.851171	49.303220
1014.407637	139.641248	49.308225
1010.874164	144.624044	49.313229
1007.454970	148.914438	49.318234
1004.426550	138.578987	49.323239
1000.704000	142.676828	49.328244
997.180926	126.055954	49.333249
993.761367	129.535364	49.338253
989.499292	136.991699	49.343258
986.330479	138.683029	49.348263
982.830709	145.488195	49.353268
979.491568	134.503807	49.358273
976.143659	129.352150	49.363277
972.669438	141.595222	49.368282
968.585943	136.190677	49.373287
965.095471	140.200830	49.378292
961.819005	135.610825	49.383297
958.385287	132.518363	49.388301
955.404559	133.982456	49.393306
951.649284	132.872137	49.398311
947.558553	135.317049	49.403316
944.585355	134.962047	49.408321
940.699214	144.303760	49.413325
937.202513	137.235745	49.418330
933.683997	131.697735	49.423335
930.482230	135.551433	49.428340
927.426717	130.146621	49.433345
923.170464	134.746604	49.438349
919.935174	145.051234	49.443354
916.438970	134.326326	49.448359
912.665897	138.167571	49.453364
909.332934	133.650888	49.458369
905.941724	143.158227	49.463373
902.693286	138.708870	49.468378
899.306954	139.734314	49.473383
895.179044	144.176147	49.478388
892.111196	136.080161	49.483393
888.268823	141.699042	49.488397
884.456787	141.767973	49.493402
881.046899	138.248346	49.498407
877.693043	142.865271	49.503412
874.397840	134.469264	49.508417
870.938880	138.509006	49.513421
866.895443	129.122019	49.518426
864.094829	135.766236	49.523431
860.329863	134.807967	49.528436
857.035617	141.184160	49.533441
853.408722	137.638486	49.538445
849.775949	141.669303	49.543450
846.796936	128.403666	49.548455
842.579336	136.134765	49.553460
839.435354	119.944882	49.558465
835.954536	143.065471	49.563469
832.009007	140.766006	49.568474
828.795447	135.935014	49.573479
825.307039	128.833759	49.578484
821.916406	129.176600	49.583489
818.116960	135.784781	49.588493
814.524354	129.001906	49.593498
811.285349	131.443791	49.598503
807.762560	133.005145	49.603508
804.572360	133.405421	49.608513
801.177710	136.111442	49.613517
797.175056	131.391669	49.618522
793.873743	139.207648	49.623527
789.802571	133.798675	49.628532
786.736275	134.818623	49.633537
783.498374	130.432542	49.638541
779.628940	128.367604	49.643546
776.333801	126.528533	49.648551
772.613111	131.448344	49.653556
769.184897	123.070290	49.658561
765.684741	133.010538	49.663565
762.150660	130.618012	49.668570
758.891296	119.825464	49.673575
755.012702	141.769674	49.678580
751.542151	131.020743	49.683585
748.052977	134.800552	49.688589
744.464695	135.523460	49.693594
741.347862	128.197612	49.698599
737.507622	133.674966	49.703604
734.601330	126.522088	49.708609
730.856063	135.708637	49.713613
726.954873	134.135824	49.718618
723.839588	135.684687	49.723623
720.226016	124.966949	49.728628
716.640331	126.953184	49.733633
713.163336	133.704055	49.738637
709.601305	120.595573	49.743642
706.528025	134.815688	49.748647
702.911380	130.261843	49.753652
699.335296	134.435147	49.758657
695.871822	136.936551	49.763661
692.091894	136.567778	49.768666
688.814712	127.187206	49.773671
684.768954	133.811773	49.778676
681.408651	131.619670	49.783681
678.000976	133.805788	49.788685
674.475956	129.040657	49.793690
671.044259	128.873982	49.798695
667.634509	129.542550	49.803700
664.324015	128.211283	49.808705
660.815020	126.197325	49.813709
657.329018	128.408060	49.818714
653.995458	123.209498	49.823719
650.037124	117.701289	49.828724
646.579717	130.452091	49.833729
642.964816	128.194004	49.838733
639.431902	134.064397	49.843738
635.775445	133.127837	49.848743
632.428335	142.194910	49.853748
629.169463	127.938563	49.858753
625.543642	132.038457	49.863757
621.928143	132.472924	49.868762
618.773104	126.269227	49.873767
615.022405	134.802202	49.878772
611.925261	120.077482	49.883777
608.082385	133.720899	49.888781
604.657982	132.344392	49.893786
601.173005	129.102834	49.898791
597.341827	133.233572	49.903796
594.283806	131.663249	49.908801
590.577134	134.701863	49.913805
587.048283	134.109693	49.918810
583.753068	125.101213	49.923815
579.850293	133.983993	49.928820
576.886297	127.255775	49.933825
573.329044	126.539260	49.938829
569.451791	121.624713	49.943834
565.874546	119.546943	49.948839
562.146482	126.120423	49.953844
558.982524	125.310227	49.958849
555.883973	125.457334	49.963853
551.866284	131.256259	49.968858
548.619936	119.072305	49.973863
544.885596	126.106430	49.978868
541.616649	119.367728	49.983873
538.113087	118.338266	49.988877
534.347508	123.868352	49.993882
531.352749	124.408758	49.998887
527.123333	123.494879	50.003892
524.065356	121.177689	50.008897
520.265254	123.899311	50.013901
516.832903	125.349431	50.018906
513.584218	125.715985	50.023911
510.190334	129.307142	50.028916
506.696790	120.631696	50.033921
503.058196	123.949393	50.038925
499.230750	134.367665	50.043930
496.115500	124.767074	50.048935
492.289602	134.033845	50.053940
489.307384	126.287699	50.058945
485.577020	124.113975	50.063949
481.639253	124.197157	50.068954
478.497558	124.080125	50.073959
474.864134	131.035643	50.078964
471.469001	118.457833	50.083969
468.251409	127.612503	50.088973
464.158172	132.797075	50.093978
461.263378	120.465229	50.098983
457.478395	134.080626	50.103988
454.027130	114.045378	50.108993
450.543804	121.238920	50.113997
446.504633	124.235787	50.119002
443.276141	124.034280	50.124007
439.786052	126.914430	50.129012
436.830534	118.837716	50.134017
432.839853	123.457145	50.139021
429.159942	123.220642	50.144026
425.794466	122.629982	50.149031
422.150652	125.079350	50.154036
418.869427	121.426133	50.159041
415.639917	128.518297	50.164045
411.888386	128.502639	50.169050
408.666666	121.748336	50.174055
404.804263	125.720812	50.179060
401.384349	127.341434	50.184065
397.929074	126.460185	50.189069
394.260062	126.688604	50.194074
391.324350	125.964878	50.199079
387.488777	127.329890	50.204084
384.186691	124.599533	50.209089
380.388282	115.030419	50.214093
376.501520	123.745538	50.219098
373.621819	121.518930	50.224103
369.467049	122.045628	50.229108
366.448969	118.738831	50.234113
363.146532	117.154668	50.239117
359.455051	128.551814	50.244122
355.554030	117.983632	50.249127
352.222901	128.347293	50.254132
348.643786	123.944037	50.259137
345.206287	125.423164	50.264141
341.796205	130.909959	50.269146
338.377684	122.403202	50.274151
334.308775	128.694459	50.279156
331.031416	119.813484	50.284161
327.844043	130.042663	50.289165
324.517498	125.637087	50.294170
320.969541	121.781036	50.299175
317.413231	120.773313	50.304180
314.089906	119.955540	50.309185
310.513457	117.361038	50.314189
306.564438	130.499310	50.319194
303.193314	127.236197	50.324199
299.359686	127.043208	50.329204
296.261948	127.450256	50.334209
292.733049	129.039670	50.339213
289.600564	124.849062	50.344218
285.842434	122.218153	50.349223
282.027119	126.061381	50.354228
278.549194	126.680956	50.359233
275.329953	134.850739	50.364237
271.860210	128.717371	50.369242
268.205727	130.060601	50.374247
264.578249	127.070444	50.379252
261.600995	121.969512	50.384257
257.990784	124.377932	50.389261
254.347105	124.673711	50.394266
250.869837	112.838265	50.399271
247.113421	112.743838	50.404276
243.620867	121.254685	50.409281
239.915120	122.028236	50.414285
236.456996	128.008107	50.419290
233.351072	117.601466	50.424295
229.412870	129.681875	50.429300
226.639811	121.859278	50.434305
223.008829	121.041991	50.439309
219.432291	127.873045	50.444314
215.844246	124.432401	50.449319
212.200314	121.999523	50.454324
208.751971	117.689197	50.459329
205.130680	123.552839	50.464333
201.430472	125.677441	50.469338
198.230107	118.642327	50.474343
194.377864	127.848769	50.479348
191.199550	118.140475	50.484353
187.736123	122.462470	50.489357
183.954491	111.207123	50.494362
180.891007	120.441444	50.499367
176.991356	126.780396	50.504372
173.630963	115.458867	50.509377
170.085454	124.802405	50.514381
166.739309	120.871636	50.519386
163.454713	111.060791	50.524391
159.415922	122.312330	50.529396
156.388411	113.512687	50.534401
152.830346	125.802932	50.539405
149.031126	123.515800	50.544410
145.748529	119.187359	50.549415
141.805609	115.271949	50.554420
138.796583	116.660761	50.559425
134.869265	114.602645	50.564429
131.330750	122.883989	50.569434
128.310043	115.083132	50.574439
124.558993	124.064095	50.579444
121.337827	113.989208	50.584449
117.946016	120.623398	50.589453
114.140127	119.718937	50.594458
110.540472	119.342338	50.599463
106.821288	123.140593	50.604468
103.567939	119.835453	50.609473
100.476367	114.700688	50.614477
96.632966	125.211304	50.619482
92.864510	112.413084	50.624487
89.405896	120.789564	50.629492
86.185050	117.316849	50.634497
82.898529	111.512464	50.639501
78.843600	118.483614	50.644506
75.505809	115.810529	50.649511
71.919330	126.110296	50.654516
68.847282	119.108900	50.659521
65.175910	121.181681	50.664525
61.592615	124.113673	50.669530
58.337663	103.789606	50.674535
54.421181	122.007176	50.679540
50.967573	112.485291	50.684545
47.630173	123.471201	50.689549
43.621389	128.253814	50.694554
40.486261	114.104412	50.699559
36.864266	123.438217	50.704564
33.593814	116.143316	50.709569
30.119037	124.009450	50.714573
26.381639	115.916113	50.719578
23.114283	114.781067	50.724583
19.399835	123.256798	50.729588
16.140742	125.457300	50.734593
12.715188	119.973179	50.739597
8.836544	122.061980	50.744602
5.582629	115.447335	50.749607
2.117423	123.098390	50.754612