Tue Jun 21 11:22:03 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.210258	79.982489	0.000000
0.034894	85.660827	0.005005
0.471241	79.203692	0.010010
-0.104999	85.558566	0.015014
0.078553	92.473954	0.020019
0.147779	75.486332	0.025024
0.044727	89.492005	0.030029
0.000686	74.472006	0.035034
-0.508492	68.677013	0.040038
-0.602877	62.202788	0.045043
-0.960492	45.299496	0.050048
-1.313095	45.083827	0.055053
-1.703402	16.055142	0.060058
-1.789647	16.737433	0.065062
-2.036597	12.993133	0.070067
-2.518814	6.612358	0.075072
-3.027112	3.967854	0.080077
-2.902620	-3.789333	0.085082
-3.318848	-3.761810	0.090086
-3.841922	-0.627554	0.095091
-4.192904	-4.247670	0.100096
-4.782614	-4.615881	0.105101
-4.610090	-8.474432	0.110106
-4.470561	-4.830669	0.115110
-4.903261	-7.635689	0.120115
-5.199308	-5.991393	0.125120
-5.728761	-2.768466	0.130125
-6.061774	-1.341823	0.135130
-6.101343	2.104271	0.140134
-6.223523	-4.102081	0.145139
-6.095438	-1.970554	0.150144
-7.118958	4.185245	0.155149
-7.386176	-2.384060	0.160154
-7.622471	4.895232	0.165158
-7.610076	-1.385107	0.170163
-7.610116	-1.604890	0.175168
-8.136184	-0.623033	0.180173
-8.630716	-6.527375	0.185178
-9.138018	-3.944710	0.190182
-9.370468	-17.183083	0.195187
-9.104963	-5.706757	0.200192
-9.660727	0.022109	0.205197
-9.437926	-7.820618	0.210202
-9.927133	-0.383813	0.215206
-10.079496	-4.940401	0.220211
-9.667599	-6.656491	0.225216
-10.214811	-4.937649	0.230221
-10.923106	-3.543779	0.235226
-11.125236	-3.297544	0.240230
-11.633680	2.625358	0.245235
-11.000849	-6.710402	0.250240
-12.245052	4.488853	0.255245
-12.485339	-3.578124	0.260250
-12.528730	6.938626	0.265254
-12.707911	-4.581130	0.270259
-12.329084	-4.442346	0.275264
-12.494671	1.138241	0.280269
-13.207017	-6.969556	0.285274
-13.855339	-5.059134	0.290278
-14.051545	6.023216	0.295283
-14.138961	-9.079896	0.300288
-14.251041	0.407494	0.305293
-14.253812	-7.173711	0.310298
-15.135901	1.362372	0.315302
-15.462933	-4.967133	0.320307
-15.331991	1.449386	0.325312
-15.545719	9.054881	0.330317
-15.550036	1.898785	0.335322
-15.722836	4.994773	0.340326
-16.090620	-1.243528	0.345331
-16.543203	-2.946902	0.350336
-16.668140	5.896949	0.355341
-16.661133	-12.666034	0.360346
-17.647244	5.270621	0.365350
-17.983979	3.427689	0.370355
-18.261056	-8.622462	0.375360
-18.526728	5.494125	0.380365
-18.672062	-3.631674	0.385370
-18.771933	0.460210	0.390374
-18.650916	-0.451338	0.395379
-18.670338	2.820332	0.400384
-18.919924	0.232051	0.405389
-19.230933	-6.085307	0.410394
-20.073636	3.829923	0.415398
-20.054978	0.197734	0.420403
-19.956505	0.220341	0.425408
-20.820638	1.719741	0.430413
-21.311100	-9.975987	0.435418
-21.680394	1.427271	0.440422
-21.524300	-2.799940	0.445427
-21.664504	-3.081957	0.450432
-21.888765	-7.619337	0.455437
-22.116830	-6.390828	0.460442
-21.751310	5.254236	0.465446
-22.561488	-2.786448	0.470451
-22.955466	0.018988	0.475456
-23.222825	-4.061536	0.480461
-23.247124	-9.051556	0.485466
-23.167670	-0.022122	0.490470
-23.662847	-0.090648	0.495475
-24.373507	-3.014014	0.500480
-24.373955	-1.337169	0.505485
-24.654590	-1.590997	0.510490
-24.843018	-0.358002	0.515494
-25.050714	-4.430842	0.520499
-25.760504	-3.551562	0.525504
-26.159491	2.382420	0.530509
-26.196550	1.711944	0.535514
-26.334602	3.286073	0.540518
-26.578210	-0.996308	0.545523
-26.604178	-7.928986	0.550528
-26.489434	0.656527	0.555533
-26.649374	-14.438514	0.560538
-27.551962	6.725886	0.565542
-28.272503	-1.644781	0.570547
-28.011543	-9.202563	0.575552
-28.117683	1.519734	0.580557
-28.347202	-7.174960	0.585562
-28.339112	-3.740115	0.590566
-28.280156	-1.988056	0.595571
-28.960943	-4.784353	0.600576
-29.893869	-3.437148	0.605581
-29.465019	-11.748322	0.610586
-29.851146	-5.480218	0.615590
-30.264538	-4.538725	0.620595
-30.278997	-3.991654	0.625600
-31.277469	1.806184	0.630605
-31.172564	-7.286656	0.635610
-31.512224	-1.463731	0.640614
-31.807994	-9.113234	0.645619
-31.515533	0.436022	0.650624
-31.676335	-8.233149	0.655629
-31.742011	-6.749939	0.660634
-32.134309	-6.137734	0.665638
-32.841068	-2.459600	0.670643
-33.114155	-8.378901	0.675648
-33.378660	-9.731778	0.680653
-33.339037	-11.910137	0.685658
-33.397400	-7.769877	0.690662
-33.381966	-1.408232	0.695667
-34.176697	-7.853473	0.700672
-34.936567	-6.742123	0.705677
-34.696545	-8.463891	0.710682
-35.017436	-9.028165	0.715686
-35.034485	-12.223661	0.720691
-34.778769	-10.574240	0.725696
-35.472857	-11.065465	0.730701
-35.941161	-10.908943	0.735706
-36.114573	-6.855795	0.740710
-36.135563	-10.787083	0.745715
-36.729909	-6.517808	0.750720
-37.336312	-6.654543	0.755725
-37.611789	-11.496802	0.760730
-37.988649	-2.313268	0.765734
-37.913857	-1.562530	0.770739
-37.953013	-6.717625	0.775744
-38.138934	2.876711	0.780749
-38.056595	-10.361694	0.785754
-38.016537	-1.062892	0.790758
-38.737160	-3.173175	0.795763
-38.685169	-7.164501	0.800768
-39.544246	4.069253	0.805773
-39.301252	-6.638531	0.810778
-40.442299	-0.977907	0.815782
-40.617804	-1.092462	0.820787
-40.633266	-12.761073	0.825792
-41.106830	-2.377730	0.830797
-41.258880	-0.019650	0.835802
-41.500373	-3.639145	0.840806
-41.623333	0.638699	0.845811
-41.515692	-1.749837	0.850816
-41.806199	-2.014658	0.855821
-41.794547	-2.060751	0.860826
-42.197260	-4.798508	0.865830
-42.957262	-3.431195	0.870835
-42.950729	-7.540497	0.875840
-43.478606	-3.012277	0.880845
-43.331818	-5.625939	0.885850
-43.374783	4.254931	0.890854
-44.225339	-8.565747	0.895859
-44.837544	-2.746035	0.900864
-44.660708	-8.407929	0.905869
-44.350499	-8.217726	0.910874
-44.497668	-3.348219	0.915878
-45.224382	1.257724	0.920883
-44.858655	-8.569561	0.925888
-45.621973	-7.908741	0.930893
-46.055593	-7.241345	0.935898
-46.108257	-7.258633	0.940902
-46.346884	-11.696937	0.945907
-46.391612	-14.794511	0.950912
-47.364907	-1.962794	0.955917
-47.551576	-6.550402	0.960922
-47.991471	1.714731	0.965926
-48.254420	-1.001574	0.970931
-48.287566	-17.494392	0.975936
-48.365018	-10.614568	0.980941
-48.222678	-1.704874	0.985946
-48.279718	-6.908116	0.990950
-48.146922	-2.061883	0.995955
-48.389208	-10.852334	1.000960
-48.935320	-3.583704	1.005965
-49.389252	0.084729	1.010970
-50.125386	-4.958892	1.015974
-50.270523	-0.606731	1.020979
-50.235297	-6.029491	1.025984
-50.412365	-1.204167	1.030989
-50.959358	-6.324496	1.035994
-51.770738	-4.025949	1.040998
-52.232739	-11.116307	1.046003
-51.525085	-8.526652	1.051008
-51.854418	-2.000369	1.056013
-51.901913	-11.123417	1.061018
-52.048851	-15.855931	1.066022
-52.342286	-8.143907	1.071027
-52.968821	-8.993227	1.076032
-53.479973	-4.527569	1.081037
-53.392256	-9.636974	1.086042
-53.660601	0.626350	1.091046
-53.690013	-2.358717	1.096051
-54.109798	-4.736869	1.101056
-54.927121	5.311703	1.106061
-55.225490	0.065544	1.111066
-55.429608	2.766726	1.116070
-55.362051	-0.862509	1.121075
-54.641128	-3.386152	1.126080
-55.622168	-6.215797	1.131085
-55.644422	-4.396025	1.136090
-56.557856	-2.018022	1.141094
-56.985371	-5.766746	1.146099
-56.920131	-0.776324	1.151104
-56.847277	-0.614894	1.156109
-57.016758	-0.248364	1.161114
-57.034436	-6.000985	1.166118
-57.848611	0.896261	1.171123
-57.910637	-7.605943	1.176128
-58.337457	2.926345	1.181133
-58.520502	-7.453365	1.186138
-58.553547	7.204458	1.191142
-58.715486	1.255897	1.196147
-59.446683	6.359270	1.201152
-59.808924	-3.021865	1.206157
-59.856540	0.498770	1.211162
-59.863029	5.899486	1.216166
-60.592253	-0.602972	1.221171
-60.408266	-7.223901	1.226176
-60.197468	-1.450101	1.231181
-60.469724	-7.283500	1.236186
-61.464517	-0.081460	1.241190
-61.728444	-1.602952	1.246195
-61.403292	-7.174363	1.251200
-61.966456	0.765063	1.256205
-62.136754	-3.372378	1.261210
-62.865151	-1.530977	1.266214
-63.097945	3.753099	1.271219
-62.929921	-1.361714	1.276224
-63.289057	5.324018	1.281229
-63.171836	-2.017959	1.286234
-63.249056	1.325244	1.291238
-64.155917	-0.762875	1.296243
-64.531869	-2.447755	1.301248
-65.046250	3.769566	1.306253
-64.997726	-7.753947	1.311258
-64.946082	-6.440137	1.316262
-65.108228	6.457352	1.321267
-64.720453	-1.070128	1.326272
-65.543835	0.351294	1.331277
-66.000267	2.127136	1.336282
-66.281811	5.271916	1.341286
-66.301153	12.900474	1.346291
-66.491008	-3.754461	1.351296
-67.499638	6.262450	1.356301
-67.509819	3.845079	1.361306
-67.761828	3.441277	1.366310
-68.170127	0.958808	1.371315
-68.067374	-5.546253	1.376320
-68.366365	-2.148170	1.381325
-68.941585	-1.776014	1.386330
-68.346925	-5.654943	1.391334
-68.194098	-5.634826	1.396339
-68.713990	0.327072	1.401344
-69.506745	8.387996	1.406349
-69.622679	1.413385	1.411354
-69.822481	-9.744982	1.416358
-70.780641	2.074485	1.421363
-71.020385	1.296878	1.426368
-71.277184	8.478136	1.431373
-70.779877	-1.199067	1.436378
-71.279013	-8.789824	1.441382
-71.491048	-0.451330	1.446387
-71.475014	-5.544128	1.451392
-71.623109	7.471012	1.456397
-72.157843	0.807490	1.461402
-72.520538	2.056323	1.466406
-73.227615	3.597803	1.471411
-72.883517	-2.609197	1.476416
-73.035393	8.791012	1.481421
-73.107573	0.034350	1.486426
-74.012809	2.589585	1.491430
-74.473846	-1.397686	1.496435
-74.331674	0.707036	1.501440
-74.735049	4.840894	1.506445
-74.825997	2.487416	1.511450
-74.581498	-0.037053	1.516454
-75.147257	2.958253	1.521459
-75.325594	-0.154492	1.526464
-76.160564	2.296163	1.531469
-75.973918	-1.352201	1.536474
-76.159150	3.746399	1.541478
-76.459162	4.561378	1.546483
-76.478321	-8.842946	1.551488
-77.678532	1.575886	1.556493
-77.789428	-5.678583	1.561498
-77.841911	-0.205922	1.566502
-77.944208	1.864497	1.571507
-78.061937	-2.063005	1.576512
-77.999651	9.307263	1.581517
-78.093277	-3.357366	1.586522
-78.084109	-7.947211	1.591526
-78.986135	7.668318	1.596531
-79.165670	3.183128	1.601536
-79.388731	3.014093	1.606541
-79.656344	0.094127	1.611546
-80.300143	5.117909	1.616550
-80.847860	2.202299	1.621555
-80.826734	5.679385	1.626560
-81.020793	0.849494	1.631565
-81.061772	1.028394	1.636570
-80.805254	0.717777	1.641574
-80.964542	-5.701658	1.646579
-81.223993	-8.211142	1.651584
-82.288371	2.419626	1.656589
-82.367854	-3.247575	1.661594
-82.584426	-0.149469	1.666598
-82.761343	-0.932152	1.671603
-82.494670	-10.245951	1.676608
-83.689168	-0.117157	1.681613
-83.862513	-1.199785	1.686618
-84.248223	-6.872510	1.691622
-84.377986	1.372836	1.696627
-84.031458	-8.868429	1.701632
-84.028554	-1.413664	1.706637
-84.335969	-3.411416	1.711642
-85.304193	6.217166	1.716646
-85.678041	3.651837	1.721651
-85.574426	-1.619647	1.726656
-85.755957	10.660050	1.731661
-85.720176	4.386496	1.736666
-85.841752	-7.752936	1.741670
-86.916401	-3.549942	1.746675
-87.534780	-1.871795	1.751680
-87.733379	4.020123	1.756685
-86.694348	-7.135615	1.761690
-87.015433	-1.826658	1.766694
-87.582339	-0.541834	1.771699
-87.627010	-0.835328	1.776704
-88.461931	-0.281041	1.781709
-88.774762	4.342993	1.786714
-88.544026	0.607210	1.791718
-89.055504	5.730241	1.796723
-88.953399	-1.087091	1.801728
-90.184676	8.636561	1.806733
-90.313757	4.040600	1.811738
-90.479899	3.230085	1.816742
-90.774369	1.434231	1.821747
-90.093881	-0.085207	1.826752
-90.454878	-1.030790	1.831757
-90.415498	0.651298	1.836762
-91.008798	4.263884	1.841766
-91.798940	3.414433	1.846771
-92.021443	2.105516	1.851776
-92.317869	1.679866	1.856781
-92.152934	-1.989767	1.861786
-92.153325	0.239401	1.866790
-92.396667	-3.340515	1.871795
-93.101497	-3.481068	1.876800
-93.782091	4.684810	1.881805
-93.680503	-3.590917	1.886810
-93.694845	3.172294	1.891814
-93.681070	1.499833	1.896819
-94.385165	4.085893	1.901824
-94.994683	-4.428250	1.906829
-95.309105	-5.677938	1.911834
-95.634115	-2.378947	1.916838
-95.726969	5.517127	1.921843
-95.243161	-0.100889	1.926848
-95.507660	-5.145845	1.931853
-95.577405	-3.525407	1.936858
-95.783197	-2.686368	1.941862
-96.652615	2.939939	1.946867
-96.842104	-4.316115	1.951872
-97.010063	-5.237032	1.956877
-96.950697	-3.824061	1.961882
-97.773040	-6.612095	1.966886
-98.663174	1.680245	1.971891
-98.243547	-2.497272	1.976896
-98.184671	-6.728114	1.981901
-98.509820	-8.319777	1.986906
-98.516873	-13.877017	1.991910
-98.870650	-2.744115	1.996915
-99.280331	-4.553113	2.006912
-99.074645	1.993264	2.016909
-98.929726	-6.813893	2.026906
-98.033053	-4.957028	2.036902
-97.516741	-0.354759	2.046899
-97.218972	-4.481552	2.056896
-96.541871	1.726535	2.066893
-95.905964	2.254163	2.076890
-95.607703	5.699727	2.086886
-94.450295	2.907315	2.096883
-94.613851	3.334589	2.106880
-94.669460	2.304384	2.116877
-93.432755	0.870276	2.126874
-93.022406	1.386062	2.136870
-92.598366	7.377027	2.146867
-91.660915	-3.900394	2.156864
-91.264739	-6.842761	2.166861
-91.323616	-1.644356	2.176858
-90.769990	-1.751574	2.186854
-89.760977	2.292328	2.196851
-89.457958	-0.495512	2.206848
-89.061387	-5.946282	2.216845
-88.668461	-0.756905	2.226842
-88.559010	-1.530912	2.236838
-87.193911	1.439224	2.246835
-86.874872	-7.071348	2.256832
-86.583115	-3.978781	2.266829
-86.249266	-0.073997	2.276826
-85.379194	0.304799	2.286822
-85.277798	-1.052330	2.296819
-84.134920	-5.063209	2.306816
-83.633991	-3.946749	2.316813
-83.841761	-4.328573	2.326810
-83.266529	-11.875864	2.336806
-82.502659	-7.236349	2.346803
-81.971319	-10.943029	2.356800
-81.204376	-0.078521	2.366797
-80.730960	-6.823355	2.376794
-80.694370	-5.269404	2.386790
-80.630271	-1.270748	2.396787
-79.299842	-3.227969	2.406784
-79.053730	-4.498811	2.416781
-77.979462	-1.695283	2.426778
-77.705648	-0.170147	2.436774
-77.889923	2.208943	2.446771
-77.402974	-3.283075	2.456768
-76.456505	-7.634661	2.466765
-76.152526	-0.970005	2.476762
-75.226830	-0.695260	2.486758
-74.700421	-2.972389	2.496755
-74.345261	0.333939	2.506752
-74.397141	-2.838901	2.516749
-73.184050	-2.164023	2.526746
-72.952222	-4.481676	2.536742
-72.925319	-0.080109	2.546739
-71.892523	-7.287063	2.556736
-71.689917	-2.418459	2.566733
-70.643675	-3.125519	2.576730
-69.985671	-13.547544	2.586726
-69.677436	-2.760790	2.596723
-69.675428	-7.323277	2.606720
-69.549190	-0.899678	2.616717
-68.769945	-12.105052	2.626714
-67.774260	-12.928612	2.636710
-66.982830	-11.886736	2.646707
-66.566330	-17.074656	2.656704
-66.648501	-12.089344	2.666701
-66.385224	-7.363171	2.676698
-65.405597	-10.696954	2.686694
-65.162723	-8.629658	2.696691
-64.449593	-10.767784	2.706688
-63.654033	-9.882683	2.716685
-63.498473	-9.824590	2.726682
-63.389790	-2.697251	2.736678
-62.621176	-0.311970	2.746675
-61.877174	-6.358102	2.756672
-60.872919	-7.313486	2.766669
-61.097833	-6.704548	2.776666
-60.813393	-6.529686	2.786662
-60.058798	-1.751307	2.796659
-59.032867	-0.676737	2.806656
-58.949965	-6.287966	2.816653
-58.657122	-7.324900	2.826650
-57.781652	-6.275007	2.836646
-57.625336	-5.436184	2.846643
-56.872530	-9.119472	2.856640
-55.917089	-10.581480	2.866637
-55.592396	-11.259736	2.876634
-55.602307	-12.474348	2.886630
-55.603811	-5.640156	2.896627
-54.399125	-8.654963	2.906624
-54.012660	-9.863098	2.916621
-52.876757	-9.701600	2.926618
-52.570401	-8.170786	2.936614
-52.661138	-4.928134	2.946611
-52.232092	-8.285732	2.956608
-51.770510	-6.572171	2.966605
-50.934109	-7.036222	2.976602
-49.719365	-0.935537	2.986598
-50.079587	-2.889787	2.996595
-49.613451	8.242684	3.006592
-49.011128	-2.439434	3.016589
-48.046852	-0.910481	3.026586
-47.702514	1.289587	3.036582
-47.711629	-1.131018	3.046579
-47.174919	0.621869	3.056576
-46.332232	2.182419	3.066573
-45.960848	-0.132658	3.076570
-45.101981	2.506002	3.086566
-44.608978	-0.503967	3.096563
-44.641496	1.511528	3.106560
-44.246918	-1.400737	3.116557
-43.416228	-2.428538	3.126554
-43.095185	2.138899	3.136550
-42.140657	-6.456362	3.146547
-41.827243	-1.839650	3.156544
-41.405761	-5.847828	3.166541
-41.018746	-2.726771	3.176538
-39.700104	-4.261369	3.186534
-39.569423	-9.970608	3.196531
-39.329918	-9.459325	3.206528
-39.527950	-1.971577	3.216525
-38.799987	-5.630398	3.226522
-38.024039	-8.429570	3.236518
-37.110975	-1.812226	3.246515
-36.851166	2.482805	3.256512
-36.652283	2.500926	3.266509
-35.677600	-1.715832	3.276506
-35.764063	-2.723345	3.286502
-34.823403	-3.995788	3.296499
-34.097246	-7.768118	3.306496
-33.974100	-3.972871	3.316493
-33.550479	-4.795939	3.326490
-32.498346	-4.476327	3.336486
-32.220707	-4.478361	3.346483
-32.304743	-8.205042	3.356480
-31.691538	-6.178323	3.366477
-31.180899	-3.546210	3.376474
-30.100421	-8.089903	3.386470
-29.831908	-2.252780	3.396467
-29.649231	-1.655423	3.406464
-28.838647	-3.136709	3.416461
-28.185665	-3.785749	3.426458
-27.998196	-4.368767	3.436454
-26.985239	-3.491206	3.446451
-26.302524	-1.841133	3.456448
-26.202702	-8.756260	3.466445
-26.212308	-2.120876	3.476442
-25.205083	-1.177361	3.486438
-24.446067	1.941176	3.496435
-24.508318	-2.495284	3.506432
-24.202371	-7.305689	3.516429
-23.194550	-2.768795	3.526426
-22.539903	-2.389484	3.536422
-22.365794	2.246151	3.546419
-22.342025	-0.424116	3.556416
-21.312791	-5.924919	3.566413
-21.027391	-9.981888	3.576410
-19.929746	-10.691125	3.586406
-19.587792	-7.671869	3.596403
-19.623881	-9.208755	3.606400
-18.907088	-6.689220	3.616397
-18.057210	-5.895103	3.626394
-17.895556	-10.848967	3.636390
-17.700916	-5.966789	3.646387
-16.534218	-1.235697	3.656384
-16.287237	-9.441713	3.666381
-16.177464	-3.597469	3.676378
-15.028679	-0.497635	3.686374
-14.721744	1.538708	3.696371
-14.475949	0.570027	3.706368
-13.585023	-2.259048	3.716365
-13.056713	-4.247617	3.726362
-13.040484	-0.928823	3.736358
-12.658135	3.281705	3.746355
-11.878912	-7.496486	3.756352
-11.427042	-4.016682	3.766349
-10.539483	-0.760571	3.776346
-10.471067	-3.261194	3.786342
-10.081871	-2.696256	3.796339
-8.890871	-3.357722	3.806336
-8.686440	0.141126	3.816333
-8.707645	0.039403	3.826330
-7.692456	0.269113	3.836326
-7.251860	2.295969	3.846323
-7.118121	-4.491211	3.856320
-5.983081	-3.183960	3.866317
-5.647432	-4.643105	3.876314
-5.273890	-5.935441	3.886310
-5.106244	-3.635178	3.896307
-4.249832	3.678759	3.906304
-3.739523	0.218595	3.916301
-3.473378	1.069860	3.926298
-2.737904	12.175330	3.936294
-2.730282	13.821217	3.946291
-2.250059	29.721681	3.956288
-2.051262	41.447941	3.966285
-1.421667	59.435892	3.976282
-0.766772	81.641297	3.986278
-0.378177	111.620608	3.996275
0.000000	120.157563	4.001280
0.152943	130.639519	4.006285
0.300800	135.408515	4.011290
0.353488	141.879690	4.016294
0.696848	158.102158	4.021299
0.619376	159.548660	4.026304
0.306714	169.738135	4.031309
0.961564	170.878076	4.036314
0.676087	176.618883	4.041318
0.998360	181.660935	4.046323
0.884026	177.935482	4.051328
0.843496	180.918434	4.056333
0.988340	166.610427	4.061338
0.706766	173.786393	4.066342
1.125085	161.420463	4.071347
1.060594	178.022473	4.076352
0.922340	177.632385	4.081357
0.747839	171.140005	4.086362
0.918512	190.221668	4.091366
1.476629	196.395853	4.096371
1.357400	202.003173	4.101376
0.753963	186.941309	4.106381
1.306204	195.947036	4.111386
1.256070	205.174074	4.116390
1.486028	194.176253	4.121395
1.582517	189.874992	4.126400
0.790249	185.517055	4.131405
1.256677	177.256786	4.136410
0.775886	177.007877	4.141414
0.864972	181.687163	4.146419
1.419285	184.678571	4.151424
1.180437	191.014717	4.156429
1.487373	189.583377	4.161434
1.003104	196.200124	4.166438
1.346381	191.144830	4.171443
1.028207	194.028520	4.176448
1.111565	195.564624	4.181453
1.129567	197.083134	4.186458
1.077969	196.067944	4.191462
1.131281	187.218755	4.196467
1.536600	192.632848	4.201472
1.030515	200.995083	4.206477
1.191508	190.335669	4.211482
1.498848	197.556209	4.216486
1.430455	197.067329	4.221491
1.268742	195.479750	4.226496
1.305414	206.091716	4.231501
1.514318	200.475149	4.236506
1.252045	207.799488	4.241510
1.832949	222.580428	4.246515
1.512357	211.235083	4.251520
1.546772	201.943630	4.256525
1.538517	198.836025	4.261530
1.360210	207.053410	4.266534
1.499800	211.570027	4.271539
1.777015	210.123873	4.276544
1.511468	217.933413	4.281549
1.787240	209.726602	4.286554
1.628703	198.214522	4.291558
1.551755	199.185956	4.296563
1.451336	203.130772	4.301568
1.367750	217.675613	4.306573
2.009350	221.643986	4.311578
1.667050	227.214252	4.316582
1.610972	218.929975	4.321587
1.744242	227.591088	4.326592
1.620270	231.119488	4.331597
1.781999	231.805719	4.336602
1.699632	234.278392	4.341606
1.668414	234.653407	4.346611
1.721011	240.944471	4.351616
1.747197	241.565136	4.356621
2.038621	242.231865	4.361626
1.780122	251.822589	4.366630
2.020030	235.016888	4.371635
2.011882	220.245366	4.376640
1.588563	218.218620	4.381645
1.770611	210.483369	4.386650
1.763951	230.517185	4.391654
1.842801	238.246817	4.396659
2.031584	244.267872	4.401664
1.651594	254.228986	4.406669
1.952953	241.439341	4.411674
1.859344	245.290688	4.416678
2.111716	241.228227	4.421683
2.154960	241.563483	4.426688
1.865117	231.871833	4.431693
1.742978	231.663978	4.436698
2.090243	233.347406	4.441702
1.813783	232.771618	4.446707
2.130234	228.107531	4.451712
1.833861	234.380996	4.456717
2.207267	232.560156	4.461722
2.066793	234.891885	4.466726
2.022335	235.519313	4.471731
1.469406	228.591696	4.476736
1.842584	228.393187	4.481741
2.012882	232.709955	4.486746
1.996487	229.154557	4.491750
1.854138	239.122289	4.496755
2.045875	233.958675	4.501760
1.760872	237.700420	4.506765
2.361244	236.405982	4.511770
2.064232	235.018996	4.516774
1.977781	239.207389	4.521779
2.248778	229.290065	4.526784
1.908876	250.077852	4.531789
1.744875	244.925781	4.536794
2.140586	250.843112	4.541798
2.010387	253.263522	4.546803
2.402003	255.482479	4.551808
2.039486	258.456207	4.556813
2.353582	258.638276	4.561818
2.426400	260.810368	4.566822
2.303208	256.127904	4.571827
2.372989	248.204417	4.576832
2.455272	257.442119	4.581837
2.276982	251.255413	4.586842
2.363397	264.774617	4.591846
2.476981	256.299029	4.596851
2.634620	255.834485	4.601856
2.355300	252.882066	4.606861
2.359201	257.873655	4.611866
2.028128	259.213171	4.616870
2.150866	257.953026	4.621875
2.391545	251.480269	4.626880
2.119501	250.922693	4.631885
2.440163	258.409038	4.636890
2.244072	267.693434	4.641894
2.409000	267.047318	4.646899
2.678646	265.248984	4.651904
2.266470	271.576963	4.656909
2.502455	268.063237	4.661914
2.461174	270.905038	4.666918
2.348507	269.125610	4.671923
2.580985	263.257856	4.676928
2.653043	259.871129	4.681933
2.320083	266.624665	4.686938
2.526400	282.502913	4.691942
2.696993	296.278753	4.696947
2.751187	292.801045	4.701952
2.700061	285.638754	4.706957
2.870071	274.419328	4.711962
2.851753	269.944456	4.716966
2.581074	271.150440	4.721971
2.598524	264.240444	4.726976
2.424425	272.791257	4.731981
2.914326	281.049391	4.736986
2.600890	286.655549	4.741990
2.829431	286.433038	4.746995
2.769956	280.419838	4.752000
2.577276	285.812217	4.757005
2.892741	283.283452	4.762010
2.863286	297.919257	4.767014
3.028034	291.477015	4.772019
2.806965	274.705769	4.777024
2.751691	278.300553	4.782029
2.816368	263.094238	4.787034
2.730012	278.319811	4.792038
2.726654	293.990857	4.797043
2.863740	295.594443	4.802048
2.624708	304.123860	4.807053
2.751051	299.639628	4.812058
2.975445	297.713214	4.817062
2.531513	296.243595	4.822067
2.725324	301.358463	4.827072
2.544965	298.626451	4.832077
2.864199	308.597518	4.837082
2.783855	305.448745	4.842086
2.582729	302.870541	4.847091
2.642506	297.964378	4.852096
3.187211	321.273369	4.857101
3.189343	318.402403	4.862106
2.975177	324.078964	4.867110
3.044121	327.328770	4.872115
3.288238	318.524872	4.877120
3.103237	312.601118	4.882125
2.979683	303.354903	4.887130
3.139171	317.022882	4.892134
3.123171	313.827932	4.897139
3.194730	308.004371	4.902144
2.894120	307.593803	4.907149
3.187833	310.227401	4.912154
3.606814	322.427450	4.917158
3.102761	314.281633	4.922163
2.943422	307.176521	4.927168
3.074297	327.456460	4.932173
3.403435	318.908637	4.937178
3.135493	323.954536	4.942182
3.121449	335.367886	4.947187
3.511960	329.042167	4.952192
3.063811	326.290753	4.957197
3.397022	324.032947	4.962202
3.323703	331.007159	4.967206
3.346516	322.040791	4.972211
3.343392	319.785595	4.977216
3.087626	324.593859	4.982221
3.515387	330.838031	4.987226
3.471287	319.101288	4.992230
3.368126	329.115869	4.997235
3.614296	325.508683	5.002240
3.131620	327.466897	5.007245
3.228733	324.139549	5.012250
3.135327	332.793659	5.017254
3.081005	329.194197	5.022259
3.326958	322.721129	5.027264
3.169929	328.729229	5.032269
2.910751	329.123444	5.037274
3.068122	323.954046	5.042278
3.164347	327.402196	5.047283
3.407549	349.378221	5.052288
3.480555	361.490943	5.057293
3.827372	365.455084	5.062298
3.496194	363.434372	5.067302
3.314447	363.763275	5.072307
3.625651	362.899543	5.077312
3.798153	372.825882	5.082317
3.718640	355.316551	5.087322
3.751333	371.958128	5.092326
3.730301	356.259152	5.097331
3.438420	337.830291	5.102336
3.244779	356.179588	5.107341
3.767355	358.386149	5.112346
3.861562	370.963254	5.117350
3.940215	365.892915	5.122355
4.013947	352.941956	5.127360
3.426831	347.002880	5.132365
3.741968	328.998430	5.137370
3.757167	348.182205	5.142374
3.922122	342.387172	5.147379
3.993583	330.639769	5.152384
3.628819	335.097263	5.157389
3.646225	328.892723	5.162394
3.517911	333.246731	5.167398
3.484666	358.737329	5.172403
3.851466	362.458790	5.177408
3.531105	361.620310	5.182413
3.720604	368.477610	5.187418
3.934922	361.373155	5.192422
3.943286	363.117057	5.197427
4.070915	346.142358	5.202432
3.532893	363.583713	5.207437
3.663666	352.708173	5.212442
3.715685	359.876149	5.217446
3.383806	365.627275	5.222451
3.769125	358.220997	5.227456
3.944429	361.027344	5.232461
3.823720	364.402495	5.237466
4.263112	352.706632	5.242470
3.880216	364.506884	5.247475
4.123419	365.716190	5.252480
3.642272	370.146788	5.257485
3.841344	369.849234	5.262490
4.100059	381.740396	5.267494
4.192432	381.123064	5.272499
4.163396	393.206333	5.277504
4.057734	395.827735	5.282509
4.139446	381.010198	5.287514
4.009851	376.761913	5.292518
4.288187	385.124400	5.297523
4.211893	372.643855	5.302528
3.875634	372.568543	5.307533
3.859642	377.668448	5.312538
4.386520	395.086241	5.317542
4.434395	389.362674	5.322547
4.460868	389.869039	5.327552
4.182727	374.581640	5.332557
4.250719	365.855226	5.337562
4.026227	368.006313	5.342566
4.274187	376.704760	5.347571
4.439119	384.681682	5.352576
4.308963	371.698361	5.357581
4.378173	372.948910	5.362586
4.109716	364.713930	5.367590
4.280669	382.419360	5.372595
4.400237	385.965484	5.377600
4.327922	378.956634	5.382605
4.542896	378.847272	5.387610
4.235819	368.742798	5.392614
3.901050	365.770332	5.397619
4.086962	371.672919	5.402624
4.063438	390.103214	5.407629
4.265873	394.294922	5.412634
4.235389	394.833807	5.417638
4.102161	400.882986	5.422643
4.513177	391.607006	5.427648
4.011812	394.081597	5.432653
4.113023	394.769371	5.437658
4.304990	395.970981	5.442662
4.671671	416.488264	5.447667
4.716568	406.332191	5.452672
4.289382	403.764763	5.457677
4.708575	401.269322	5.462682
4.201743	403.081371	5.467686
4.622990	415.046682	5.472691
4.826646	417.069848	5.477696
4.567205	416.260349	5.482701
4.470066	402.772467	5.487706
4.666287	423.728842	5.492710
4.486129	417.494031	5.497715
4.844822	420.401844	5.502720
4.406460	418.472283	5.507725
4.566641	422.785846	5.512730
4.690349	426.448907	5.517734
4.767126	424.222498	5.522739
4.816209	421.461943	5.527744
4.418112	434.245928	5.532749
4.823065	428.087093	5.537754
4.588724	429.823239	5.542758
4.473760	426.411203	5.547763
4.673785	425.627842	5.552768
4.534744	428.661885	5.557773
4.952434	429.403620	5.562778
4.685244	423.082576	5.567782
4.646321	436.408969	5.572787
4.935567	427.283769	5.577792
4.826517	432.162296	5.582797
4.868904	428.045954	5.587802
4.919732	430.308540	5.592806
4.854294	431.091598	5.597811
5.238231	427.064137	5.602816
4.872939	433.274698	5.607821
4.981138	430.404499	5.612826
4.887070	429.197015	5.617830
4.598954	435.731258	5.622835
4.981281	429.349033	5.627840
4.595325	442.907145	5.632845
4.906094	432.801950	5.637850
4.846356	433.254707	5.642854
4.902203	440.375317	5.647859
4.960938	438.007442	5.652864
4.768021	436.725748	5.657869
5.179562	429.212676	5.662874
4.897849	438.824330	5.667878
4.939939	436.755218	5.672883
4.909389	439.632175	5.677888
5.027069	453.707596	5.682893
5.133892	456.116219	5.687898
5.327776	462.403712	5.692902
4.765468	449.541022	5.697907
5.221268	456.440304	5.702912
5.085417	468.060801	5.707917
4.877890	456.966117	5.712922
5.175257	459.180385	5.717926
4.930074	466.479913	5.722931
5.302525	466.436434	5.727936
5.014268	471.904694	5.732941
5.350450	463.234065	5.737946
5.405626	464.980094	5.742950
5.360175	468.068110	5.747955
5.365751	470.522509	5.752960
4.900596	467.652325	5.757965
5.355125	465.615754	5.762970
5.095415	462.338386	5.767974
4.960004	464.983473	5.772979
5.248097	466.871695	5.777984
5.094275	470.255904	5.782989
4.949605	455.618655	5.787994
5.221886	458.781339	5.792998
5.043361	463.808728	5.798003
5.345963	481.096808	5.803008
5.476095	490.682132	5.808013
5.672113	484.471636	5.813018
5.277975	474.320926	5.818022
5.054253	482.969860	5.823027
5.569613	483.018949	5.828032
5.522885	502.420573	5.833037
5.153048	495.387922	5.838042
5.346279	492.438904	5.843046
5.310054	499.441387	5.848051
5.711049	499.601373	5.853056
5.688459	496.807286	5.858061
5.811627	499.053364	5.863066
5.400092	502.162144	5.868070
5.412275	497.801151	5.873075
5.625700	494.289335	5.878080
5.692335	494.330043	5.883085
5.525281	492.519535	5.888090
5.573745	498.046701	5.893094
5.806621	505.959351	5.898099
6.023573	490.396266	5.903104
5.758638	495.990324	5.908109
5.856517	490.546357	5.913114
5.943517	480.817212	5.918118
5.438616	471.070642	5.923123
5.552454	470.519017	5.928128
5.685070	481.454903	5.933133
5.770524	489.723485	5.938138
5.718478	490.343497	5.943142
5.664420	492.414676	5.948147
5.615442	488.386857	5.953152
5.765391	495.744109	5.958157
5.931276	489.180430	5.963162
6.022934	503.385319	5.968166
6.082013	498.580442	5.973171
6.035571	480.484330	5.978176
5.753839	471.912859	5.983181
5.450920	463.491325	5.988186
5.838919	478.871209	5.993190
5.336996	488.255714	5.998195
5.726670	494.066787	6.003200
5.908301	498.790638	6.008205
6.033147	495.939379	6.013210
6.124024	494.075899	6.018214
5.696909	498.423584	6.023219
5.919773	500.100409	6.028224
6.015771	502.618776	6.033229
6.289966	504.479309	6.038234
5.894195	503.829728	6.043238
5.830805	506.621557	6.048243
5.833316	499.342933	6.053248
5.759449	508.102836	6.058253
5.771744	504.849880	6.063258
6.034558	504.785680	6.068262
5.710482	504.138435	6.073267
5.891184	497.808908	6.078272
5.908234	504.924526	6.083277
5.896918	509.329857	6.088282
6.050988	500.220289	6.093286
6.016340	512.499946	6.098291
5.997006	496.144790	6.103296
5.773587	503.376992	6.108301
6.064564	501.855912	6.113306
5.767421	484.363725	6.118310
5.718594	493.844495	6.123315
6.028217	494.744042	6.128320
5.967198	496.179563	6.133325
5.669949	487.154602	6.138330
6.055435	500.273030	6.143334
5.671449	502.534217	6.148339
5.814379	493.688957	6.153344
5.596613	503.857411	6.158349
5.655936	509.544995	6.163354
5.617481	498.200083	6.168358
5.602478	506.913533	6.173363
5.647021	498.891678	6.178368
5.637020	507.374598	6.183373
5.631397	506.348617	6.188378
5.782931	506.193321	6.193382
5.575751	501.281173	6.198387
5.981074	501.594565	6.203392
5.752280	517.609831	6.208397
5.705511	501.927599	6.213402
5.829988	514.969671	6.218406
5.956967	524.862204	6.223411
6.004671	529.622253	6.228416
5.672392	520.316932	6.233421
6.105320	532.802164	6.238426
6.128502	519.443840	6.243430
5.908322	509.944529	6.248435
6.249437	495.719556	6.253440
5.973784	499.980789	6.258445
6.033721	506.655557	6.263450
5.911185	508.962254	6.268454
5.779206	495.224310	6.273459
5.870909	490.191040	6.278464
5.875855	496.156596	6.283469
6.269051	499.829911	6.288474
6.076156	501.387320	6.293478
5.734033	504.121700	6.298483
5.891220	501.791781	6.303488
5.890891	504.565668	6.308493
5.925410	493.201571	6.313498
6.041896	497.265258	6.318502
5.926714	498.653704	6.323507
6.126586	503.217652	6.328512
5.549392	501.723112	6.333517
5.675382	500.013070	6.338522
5.907460	503.704776	6.343526
5.854955	512.049101	6.348531
6.326282	497.983722	6.353536
5.830961	502.474722	6.358541
5.836676	499.288176	6.363546
5.989263	500.731346	6.368550
6.017040	508.847276	6.373555
6.084529	501.523554	6.378560
5.834422	507.974571	6.383565
5.679393	496.572001	6.388570
6.164571	502.735892	6.393574
5.674391	500.715836	6.398579
5.659280	503.842645	6.403584
5.656878	505.285233	6.408589
5.804525	497.281235	6.413594
6.044177	500.999512	6.418598
5.850132	506.536842	6.423603
6.026086	498.775619	6.428608
5.770722	503.927043	6.433613
5.605741	506.006922	6.438618
5.631501	507.272570	6.443622
5.657579	507.419453	6.448627
6.148459	500.151526	6.453632
5.590576	505.820737	6.458637
5.830885	504.707658	6.463642
6.125072	498.004130	6.468646
5.758236	513.900166	6.473651
6.026390	506.384159	6.478656
6.006139	505.475452	6.483661
5.714461	504.623925	6.488666
6.108545	505.992177	6.493670
5.635046	504.579136	6.498675
5.537759	500.899525	6.503680
5.514837	507.553676	6.508685
5.669133	510.881347	6.513690
6.246957	523.323634	6.518694
5.997891	524.682745	6.523699
5.668212	508.562097	6.528704
5.757254	508.200470	6.533709
5.642608	521.876134	6.538714
5.663965	519.590215	6.543718
5.967752	531.249654	6.548723
5.947965	530.598593	6.553728
5.970903	539.336169	6.558733
6.151385	527.270017	6.563738
6.234763	515.041559	6.568742
5.808135	495.328242	6.573747
6.083006	494.566821	6.578752
5.685825	497.971994	6.583757
5.477899	490.356631	6.588762
5.683601	505.574323	6.593766
5.647939	519.390633	6.598771
5.901700	517.706398	6.603776
5.978389	529.351935	6.608781
5.328331	528.350571	6.613786
5.634403	525.683607	6.618790
5.331029	521.146737	6.623795
5.724530	519.881993	6.628800
5.931774	520.305936	6.633805
6.014473	531.790043	6.638810
5.864192	517.986633	6.643814
5.760867	523.774367	6.648819
5.985537	519.201565	6.653824
5.791085	530.467524	6.658829
5.795970	526.620222	6.663834
5.818971	524.720024	6.668838
5.661777	529.057951	6.673843
6.198825	524.045452	6.678848
5.525336	533.303285	6.683853
5.759912	521.388222	6.688858
6.079207	524.566816	6.693862
5.769163	530.454892	6.698867
6.095669	520.471555	6.703872
5.922936	528.226020	6.708877
5.761301	523.636472	6.713882
5.951506	520.482915	6.718886
6.189128	531.109782	6.723891
6.025676	521.606201	6.728896
5.594487	535.003157	6.733901
6.050859	523.788033	6.738906
5.938566	527.827450	6.743910
5.921544	522.667524	6.748915
5.872928	525.119657	6.753920
5.737682	529.430861	6.758925
5.852019	520.775228	6.763930
6.037328	524.719384	6.768934
5.580960	530.258917	6.773939
5.841206	525.138723	6.778944
5.803588	537.445138	6.783949
5.768802	533.958823	6.788954
5.989194	540.340233	6.793958
5.948440	544.938316	6.798963
6.053865	535.089458	6.803968
5.763145	541.412234	6.808973
6.017105	540.064624	6.813978
5.773364	536.551932	6.818982
5.932781	540.747843	6.823987
5.916620	548.979409	6.828992
6.033572	545.628206	6.833997
5.884987	537.561743	6.839002
6.039263	541.238122	6.844006
6.007313	543.360310	6.849011
6.099277	541.126633	6.854016
5.971403	549.924314	6.859021
6.197215	541.703104	6.864026
6.182505	535.915450	6.869030
5.964339	540.298800	6.874035
6.224483	535.334123	6.879040
5.806929	541.490034	6.884045
5.807513	540.006381	6.889050
5.789118	540.440258	6.894054
5.765103	542.679930	6.899059
5.963402	538.763497	6.904064
5.540314	541.163973	6.909069
6.160881	536.449634	6.914074
5.973284	543.400240	6.919078
5.698335	538.928120	6.924083
5.802429	538.443821	6.929088
5.646358	542.679147	6.934093
5.854812	540.628848	6.939098
5.974100	532.140917	6.944102
5.830053	539.242574	6.949107
6.164779	538.851118	6.954112
5.962570	552.605444	6.959117
6.191416	534.675431	6.964122
5.915357	537.955374	6.969126
5.655801	548.180506	6.974131
6.466098	530.767348	6.979136
5.945966	538.025017	6.984141
5.862168	532.440026	6.989146
5.646129	528.809279	6.994150
5.844492	535.018505	6.999155
6.126754	527.213813	7.004160
5.991690	541.473052	7.009165
5.949109	531.905838	7.014170
5.969806	514.006368	7.019174
5.424723	513.061427	7.024179
5.943116	527.367952	7.029184
5.810614	531.674953	7.034189
5.583601	539.241071	7.039194
5.867978	539.731968	7.044198
5.741696	539.407969	7.049203
6.032328	531.061377	7.054208
5.776765	538.751219	7.059213
5.944257	545.408785	7.064218
5.776514	541.129079	7.069222
5.571293	544.749544	7.074227
6.191934	536.408689	7.079232
5.974139	544.064455	7.084237
5.807671	556.383537	7.089242
5.710743	543.533891	7.094246
5.852663	541.011721	7.099251
6.015394	545.936056	7.104256
5.763996	549.870833	7.109261
6.007190	544.708464	7.114266
6.112040	543.717469	7.119270
5.991815	544.440141	7.124275
6.279462	542.215503	7.129280
6.339679	536.963255	7.134285
5.898831	522.499902	7.139290
5.811966	511.337443	7.144294
5.652473	517.241039	7.149299
6.259795	508.951937	7.154304
5.982579	512.706469	7.159309
5.819977	512.778032	7.164314
5.983442	511.797856	7.169318
5.732504	510.882552	7.174323
6.161428	503.235138	7.179328
5.967954	518.771141	7.184333
5.875996	509.892541	7.189338
5.758700	518.957031	7.194342
5.785566	511.200558	7.199347
6.019468	506.057105	7.204352
5.997393	514.943416	7.209357
5.945993	511.068929	7.214362
5.946458	503.694932	7.219366
5.663854	514.016411	7.224371
5.807621	519.878869	7.229376
5.698907	505.716139	7.234381
5.657002	512.696677	7.239386
5.943645	510.394458	7.244390
5.911470	511.258643	7.249395
5.607989	503.690079	7.254400
5.649038	519.173237	7.259405
5.695222	529.112107	7.264410
5.725868	542.146256	7.269414
5.875008	540.825476	7.274419
6.111238	542.378728	7.279424
6.070440	536.180192	7.284429
6.058599	534.351871	7.289434
5.875460	530.714491	7.294438
5.885702	527.378594	7.299443
6.129408	523.036485	7.304448
5.756278	518.116685	7.309453
5.384329	515.242109	7.314458
5.739263	530.876759	7.319462
5.585869	532.971891	7.324467
5.503001	539.396808	7.329472
5.980043	534.562375	7.334477
5.833212	540.133142	7.339482
5.908242	541.831689	7.344486
5.809927	543.862447	7.349491
6.161654	536.242798	7.354496
5.630714	546.778486	7.359501
5.812719	549.976463	7.364506
6.062502	544.095477	7.369510
6.058179	541.419917	7.374515
6.032613	537.383078	7.379520
6.011088	543.198321	7.384525
5.892410	545.410846	7.389530
6.254475	546.729347	7.394534
5.672579	553.317021	7.399539
5.866978	539.015069	7.404544
6.119097	541.097125	7.409549
5.903297	543.812568	7.414554
6.045268	543.450464	7.419558
5.549504	544.459696	7.424563
6.055413	541.897382	7.429568
5.571502	542.840121	7.434573
5.423660	536.523737	7.439578
5.668993	536.105840	7.444582
5.322689	543.579626	7.449587
5.968213	535.236230	7.454592
5.860611	535.682510	7.459597
5.663808	534.218715	7.464602
5.819204	533.003857	7.469606
5.887650	537.328103	7.474611
6.230544	532.547853	7.479616
5.565120	545.242795	7.484621
5.704248	541.838190	7.489626
5.657054	545.010379	7.494630
5.642537	544.042703	7.499635
5.947036	540.564735	7.504640
5.683671	549.532856	7.509645
6.145093	562.615082	7.514650
6.081046	546.592492	7.519654
5.823011	543.969797	7.524659
6.044463	538.520152	7.529664
5.525483	532.532621	7.534669
5.714924	538.203801	7.539674
6.126199	551.864631	7.544678
5.869333	552.582697	7.549683
6.058709	548.127819	7.554688
6.080996	550.823178	7.559693
6.031977	555.162934	7.564698
5.921643	546.010883	7.569702
5.907574	547.238729	7.574707
6.003242	541.310248	7.579712
5.974740	547.154671	7.584717
6.045390	538.873707	7.589722
5.921953	539.671505	7.594726
5.972624	542.492801	7.599731
5.864165	542.321749	7.604736
5.958375	543.074232	7.609741
6.201318	537.334097	7.614746
6.320642	536.458715	7.619750
5.988293	542.913893	7.624755
6.060779	535.686813	7.629760
6.129269	545.057018	7.634765
5.974757	528.717305	7.639770
6.046204	517.633019	7.644774
5.615975	519.671177	7.649779
6.159728	516.960121	7.654784
5.880554	517.928948	7.659789
5.719806	508.801647	7.664794
5.748178	516.336122	7.669798
5.997640	525.957162	7.674803
5.847585	526.827054	7.679808
5.868534	533.785945	7.684813
5.959489	524.773445	7.689818
6.069323	524.859492	7.694822
5.487141	521.976707	7.699827
5.667894	523.557694	7.704832
5.878056	541.923819	7.709837
5.755600	533.885790	7.714842
6.076141	535.496715	7.719846
5.714845	539.803715	7.724851
6.107812	538.391054	7.729856
5.928329	542.312343	7.734861
5.964601	534.362487	7.739866
6.339065	538.939174	7.744870
5.631306	528.872526	7.749875
5.819490	517.596633	7.754880
5.761309	539.014635	7.759885
6.060932	541.327408	7.764890
6.089773	531.217328	7.769894
5.681771	523.220470	7.774899
5.774994	515.244024	7.779904
6.183515	530.842766	7.784909
6.047025	532.565285	7.789914
6.007570	517.622835	7.794918
5.923079	512.447641	7.799923
6.149133	505.138116	7.804928
5.962536	517.603375	7.809933
5.874886	509.227276	7.814938
5.686896	502.076694	7.819942
5.705997	518.544654	7.824947
5.909540	510.835690	7.829952
5.573444	517.218857	7.834957
5.707525	508.681916	7.839962
6.038666	509.887131	7.844966
5.597348	521.377289	7.849971
5.785418	528.167407	7.854976
5.930567	534.490626	7.859981
5.857189	546.983930	7.864986
6.211127	537.291457	7.869990
6.129972	526.103177	7.874995
6.163422	516.677307	7.880000
6.252701	511.801908	7.885005
5.984029	511.557927	7.890010
6.038135	511.411462	7.895014
5.961596	519.108552	7.900019
5.707670	513.455240	7.905024
5.784578	506.875897	7.910029
5.887030	512.074834	7.915034
5.894015	511.115637	7.920038
5.658404	517.650495	7.925043
5.879700	509.881955	7.930048
6.091304	512.963725	7.935053
6.190932	509.662365	7.940058
6.276848	513.717305	7.945062
5.993474	519.771659	7.950067
6.225865	510.848625	7.955072
6.072362	517.582421	7.960077
5.913302	517.718124	7.965082
6.274832	508.663592	7.970086
5.790717	494.899300	7.975091
5.552235	484.696957	7.980096
5.734588	494.397565	7.985101
5.707445	504.252260	7.990106
6.063801	505.272339	7.995110
5.736234	511.192516	8.000115
5.888666	505.933061	8.005133
5.919654	512.243630	8.010150
6.029326	508.645663	8.015168
5.988776	510.532392	8.020186
5.865851	511.030112	8.025203
6.147106	506.549468	8.030221
5.858114	511.364912	8.035238
5.631497	513.134628	8.040256
5.914205	510.913020	8.045274
5.685670	516.544572	8.050291
6.100960	511.982878	8.055309
6.237038	516.498623	8.060326
5.951166	518.497623	8.065344
5.940798	513.215134	8.070362
5.697755	517.883414	8.075379
5.812245	509.534222	8.080397
5.577148	517.460388	8.085414
5.982530	511.976979	8.090432
6.052828	508.759519	8.095450
5.887236	511.760768	8.100467
6.098084	509.428037	8.105485
5.705666	513.837608	8.110502
5.788434	510.211618	8.115520
5.753706	513.156357	8.120538
5.683429	522.479338	8.125555
5.657793	517.702487	8.130573
6.082176	517.211026	8.135590
5.844846	517.684189	8.140608
5.846754	520.889970	8.145626
6.274464	539.258948	8.150643
6.121407	531.553018	8.155661
6.235272	514.909666	8.160678
5.863741	526.549881	8.165696
6.304435	507.399256	8.170714
5.893753	514.304968	8.175731
6.159978	513.794030	8.180749
6.182823	517.145151	8.185766
5.833041	511.768089	8.190784
6.430466	514.557172	8.195802
5.608554	518.000934	8.200819
5.819367	524.006554	8.205837
6.081640	536.176227	8.210854
5.905819	542.565736	8.215872
6.067889	534.149010	8.220890
6.293600	549.770358	8.225907
5.881111	544.434177	8.230925
6.221833	536.216198	8.235942
6.284989	546.052687	8.240960
6.191646	547.300966	8.245978
6.126762	551.958652	8.250995
6.379295	548.611213	8.256013
6.211736	540.250641	8.261030
6.150345	536.428453	8.266048
6.530525	534.713694	8.271066
6.325358	523.421586	8.276083
6.098098	504.813623	8.281101
6.219427	512.871894	8.286118
5.833468	514.185945	8.291136
6.052300	515.691167	8.296154
6.215278	523.107359	8.301171
6.321221	524.842086	8.306189
6.297807	526.578549	8.311206
5.908391	519.108008	8.316224
6.190101	533.695735	8.321242
6.699359	538.774843	8.326259
6.494914	528.938212	8.331277
6.249289	514.572725	8.336294
6.144308	514.332491	8.341312
6.331870	502.667122	8.346330
6.188649	503.004042	8.351347
6.270437	505.323825	8.356365
6.165882	507.944915	8.361382
6.081799	511.416489	8.366400
6.511471	502.273631	8.371418
5.950057	513.204390	8.376435
5.870394	509.660017	8.381453
6.389326	523.662629	8.386470
6.222114	537.722182	8.391488
6.289127	541.076229	8.396506
6.215216	538.058811	8.401523
6.369822	541.270017	8.406541
6.741249	534.334654	8.411558
6.119531	528.597921	8.416576
6.155964	517.417571	8.421594
6.178874	529.912090	8.426611
6.205610	535.335840	8.431629
6.533207	538.718976	8.436646
6.226508	545.185862	8.441664
6.477733	535.852077	8.446682
6.184824	535.447109	8.451699
5.979917	542.246718	8.456717
6.322850	537.689912	8.461734
6.033344	545.831976	8.466752
6.216094	539.224484	8.471770
6.402467	544.338557	8.476787
6.452403	546.797666	8.481805
6.537156	537.295987	8.486822
6.218767	545.540661	8.491840
6.690926	534.806220	8.496858
6.334747	545.492207	8.501875
6.363048	546.950641	8.506893
6.622059	553.867122	8.511910
6.510898	547.374629	8.516928
6.524289	542.424785	8.521946
6.150648	554.711386	8.526963
6.305420	548.111083	8.531981
6.293298	540.706196	8.536998
6.482244	546.382400	8.542016
6.454809	549.750908	8.547034
6.084025	549.423594	8.552051
6.453956	548.576018	8.557069
6.651651	541.953650	8.562087
6.178695	546.648790	8.567104
6.490616	547.332361	8.572122
6.348999	548.106583	8.577139
6.309391	542.830697	8.582157
6.538088	535.124735	8.587175
6.202372	542.533363	8.592192
6.547379	534.517218	8.597210
6.643019	542.300645	8.602227
6.516487	545.394441	8.607245
6.801052	532.393793	8.612263
6.555103	543.057195	8.617280
6.586310	539.475757	8.622298
6.418340	543.849352	8.627315
6.370747	547.801469	8.632333
6.374122	546.873065	8.637351
6.360315	548.713248	8.642368
6.589673	565.501441	8.647386
6.818824	568.901870	8.652403
6.469939	577.459462	8.657421
6.735301	573.476867	8.662439
6.268372	579.876802	8.667456
6.704795	572.935580	8.672474
6.568021	571.469792	8.677491
6.659568	579.081683	8.682509
6.623192	576.556038	8.687527
6.619077	580.602335	8.692544
6.921364	580.268678	8.697562
6.549494	562.464260	8.702579
6.586416	562.970747	8.707597
7.061014	556.190719	8.712615
6.414375	550.608093	8.717632
6.403824	545.921052	8.722650
6.691176	558.336571	8.727667
6.583164	572.249945	8.732685
6.777329	570.656134	8.737703
6.733286	574.011454	8.742720
6.620983	567.975211	8.747738
6.895612	579.589960	8.752755
6.320886	569.577823	8.757773
6.873496	568.885219	8.762791
6.423704	584.055702	8.767808
6.574298	572.632016	8.772826
6.694032	572.590576	8.777843
6.710503	578.589819	8.782861
7.168713	573.376362	8.787879
6.606796	574.549094	8.792896
6.765715	569.314927	8.797914
6.749368	574.684806	8.802931
6.735740	575.297097	8.807949
7.082407	574.964949	8.812967
6.576503	576.997046	8.817984
6.719957	574.479218	8.823002
6.953043	577.333564	8.828019
6.741683	582.435956	8.833037
6.702593	572.867958	8.838055
6.607994	579.525311	8.843072
6.723562	572.411841	8.848090
7.144223	573.419902	8.853107
6.513993	586.952670	8.858125
6.941525	581.691734	8.863143
6.793665	572.485030	8.868160
6.607816	585.781429	8.873178
6.863228	570.106438	8.878195
6.557137	575.969342	8.883213
6.882568	576.260351	8.888231
6.387935	576.194078	8.893248
6.716522	581.902287	8.898266
7.083570	574.272208	8.903283
6.845416	572.805099	8.908301
6.899796	574.267681	8.913319
6.848308	578.705456	8.918336
6.887838	574.942133	8.923354
7.026295	578.402853	8.928371
6.824446	581.203638	8.933389
6.972816	578.886163	8.938407
6.819259	578.629366	8.943424
7.035461	576.153623	8.948442
6.749965	580.768326	8.953459
6.890505	582.985288	8.958477
7.043209	570.595772	8.963495
6.776307	579.542910	8.968512
6.485481	575.980342	8.973530
6.654355	573.507909	8.978547
6.966561	581.728098	8.983565
7.133426	584.850085	8.988583
6.536333	587.056326	8.993600
6.790789	591.950691	8.998618
7.004175	593.740267	9.003635
7.028609	605.839741	9.008653
7.290642	606.584525	9.013671
6.874745	608.957601	9.018688
7.028596	609.808088	9.023706
7.186016	610.351706	9.028723
6.897495	609.987148	9.033741
6.850030	599.405434	9.038759
7.106332	611.702328	9.043776
7.316732	611.325031	9.048794
7.234255	607.263028	9.053811
7.043362	603.662057	9.058829
7.225784	587.994607	9.063847
6.863800	583.254141	9.068864
6.697338	586.297080	9.073882
7.257692	600.324003	9.078899
7.180869	602.992876	9.083917
7.112362	607.083895	9.088935
7.162898	614.689210	9.093952
6.999733	611.781038	9.098970
7.104765	604.698037	9.103987
6.866874	615.898108	9.109005
6.994482	607.752385	9.114023
6.987735	609.731357	9.119040
6.850852	604.925265	9.124058
7.061359	605.979741	9.129075
7.096272	612.717230	9.134093
7.322079	607.480831	9.139111
7.255904	613.774659	9.144128
7.464031	606.005734	9.149146
7.405278	609.659343	9.154163
7.326338	615.853127	9.159181
7.519173	615.002591	9.164199
7.353299	607.592819	9.169216
6.788931	599.731553	9.174234
7.145844	592.797386	9.179251
7.260973	609.296100	9.184269
7.274967	606.299149	9.189287
7.275515	607.422838	9.194304
7.177552	608.979346	9.199322
7.062055	598.539006	9.204339
6.957952	602.068833	9.209357
7.425194	600.061520	9.214375
7.218076	605.747428	9.219392
7.089887	601.790035	9.224410
6.949409	598.606672	9.229427
7.174903	606.273950	9.234445
7.132349	609.283582	9.239463
7.431540	600.257148	9.244480
7.120082	607.557466	9.249498
7.623881	606.252514	9.254515
7.031052	616.335458	9.259533
7.279992	615.245923	9.264551
7.257721	608.558777	9.269568
7.617354	608.660278	9.274586
7.571907	604.899995	9.279603
7.072617	617.303311	9.284621
7.077436	610.044198	9.289639
7.050990	607.131890	9.294656
6.930455	610.063694	9.299674
7.447982	608.033684	9.304691
7.262831	612.622726	9.309709
7.120462	606.249148	9.314727
7.868167	620.365530	9.319744
7.282260	611.036273	9.324762
7.423251	607.470693	9.329779
7.522583	611.574273	9.334797
7.556829	615.816378	9.339815
7.482719	612.461994	9.344832
7.059743	608.989209	9.349850
7.514486	609.667242	9.354867
7.202344	614.818024	9.359885
7.452126	631.256474	9.364903
7.586641	625.073835	9.369920
7.047904	625.860869	9.374938
7.519111	627.089879	9.379955
7.392624	642.543672	9.384973
7.318649	637.709832	9.389991
7.532887	644.903435	9.395008
7.587651	645.784503	9.400026
7.700975	639.203229	9.405043
7.593523	650.356137	9.410061
7.663206	640.424046	9.415079
7.602757	626.250416	9.420096
7.315497	628.754547	9.425114
7.561449	631.239277	9.430131
7.575179	642.983293	9.435149
7.650828	645.683812	9.440167
7.730060	618.414323	9.445184
7.788479	617.583092	9.450202
7.445747	604.385885	9.455219
7.384884	614.742329	9.460237
7.289031	611.825373	9.465255
7.441343	621.701278	9.470272
7.494416	639.804087	9.475290
7.845133	640.666462	9.480307
7.514463	635.327134	9.485325
7.440079	647.365449	9.490343
7.379013	634.446357	9.495360
7.382018	644.276138	9.500378
7.778578	638.460901	9.505395
7.683433	638.933357	9.510413
7.854510	640.454570	9.515431
8.178100	636.529045	9.520448
7.430268	639.896003	9.525466
7.637558	637.539631	9.530483
7.724306	637.126908	9.535501
7.675697	644.212077	9.540519
7.652370	645.497388	9.545536
7.657700	648.936865	9.550554
7.507919	640.089470	9.555571
7.290764	646.323081	9.560589
7.424071	643.564616	9.565607
7.703461	638.089232	9.570624
7.812103	644.657057	9.575642
7.791688	640.894589	9.580659
7.775031	639.722663	9.585677
8.024930	637.183460	9.590695
7.888728	649.509553	9.595712
7.634893	651.085183	9.600730
7.924259	642.605788	9.605747
7.737890	642.985089	9.610765
7.577902	641.316656	9.615783
7.967953	638.353289	9.620800
7.718030	648.342466	9.625818
7.852882	646.430736	9.630835
7.930826	646.928070	9.635853
7.796862	644.709892	9.640871
8.151336	642.430125	9.645888
7.941178	637.743040	9.650906
7.757449	632.528584	9.655923
7.401667	637.829109	9.660941
7.284530	640.073591	9.665959
7.806863	635.543935	9.670976
7.556013	642.158099	9.675994
7.562971	635.799346	9.681011
7.784402	643.567702	9.686029
7.514389	642.249356	9.691047
7.896460	652.970246	9.696064
8.268752	672.454194	9.701082
7.983069	650.259117	9.706099
8.175074	654.810717	9.711117
8.089690	654.833753	9.716135
7.936361	641.482718	9.721152
7.496482	644.814825	9.726170
8.107068	648.387527	9.731187
7.850708	647.733213	9.736205
7.728850	648.843909	9.741223
8.036555	655.600415	9.746240
7.819447	664.311222	9.751258
8.211799	671.566086	9.756275
8.173717	668.755687	9.761293
7.744941	662.276175	9.766311
8.112117	655.730609	9.771328
8.118784	665.748368	9.776346
8.222869	652.770223	9.781363
8.192056	647.552683	9.786381
7.862320	649.082027	9.791399
7.896513	643.208295	9.796416
7.867158	646.934992	9.801434
8.136755	642.594222	9.806451
7.741870	646.909954	9.811469
7.996257	666.569904	9.816487
7.919762	672.246804	9.821504
8.010810	670.735802	9.826522
8.487816	664.776140	9.831539
8.266378	671.122274	9.836557
8.200495	674.423558	9.841575
8.340827	656.243095	9.846592
7.959247	652.189862	9.851610
7.922957	651.764444	9.856627
7.921337	652.029301	9.861645
8.074776	665.615822	9.866663
8.232938	665.354058	9.871680
8.188013	654.110118	9.876698
8.359966	669.922170	9.881715
8.345805	672.298611	9.886733
8.124747	672.652360	9.891751
8.290228	665.762063	9.896768
7.978042	666.514932	9.901786
8.012398	669.953937	9.906803
8.434621	668.599894	9.911821
8.144055	670.694370	9.916839
8.410023	671.216079	9.921856
8.124435	676.603216	9.926874
8.009183	680.452602	9.931891
8.262429	666.149240	9.936909
8.306218	677.604071	9.941927
8.341917	671.360222	9.946944
8.372916	672.555837	9.951962
8.067483	668.493534	9.956979
8.067880	666.340303	9.961997
8.233127	677.016017	9.967015
8.126194	665.071360	9.972032
8.521767	671.909773	9.977050
8.326902	668.587970	9.982067
8.561317	666.565269	9.987085
8.057879	679.832846	9.992103
8.725857	662.100009	9.997120
8.460241	668.139305	10.002138
8.375110	665.866583	10.007155
8.372754	662.148361	10.012173
8.409798	673.944048	10.017191
8.603965	655.778292	10.022208
8.588786	664.795994	10.027226
8.699774	653.152050	10.032243
8.244570	641.778235	10.037261
7.953947	636.628325	10.042279
8.257108	634.973746	10.047296
8.211939	656.925654	10.052314
8.229418	660.758765	10.057331
8.757536	661.810846	10.062349
8.600453	665.938003	10.067367
8.941850	658.935514	10.072384
8.212825	664.076805	10.077402
8.211510	643.483949	10.082419
8.209797	651.539243	10.087437
8.231908	658.234780	10.092455
8.454078	658.829288	10.097472
8.422980	659.778705	10.102490
8.261727	674.368266	10.107507
8.549612	659.529484	10.112525
8.417041	680.057411	10.117543
8.602640	681.247897	10.122560
8.483453	670.342600	10.127578
8.668316	668.507029	10.132595
8.524186	666.073813	10.137613
8.549753	666.258386	10.142631
8.580998	665.169464	10.147648
8.548185	671.904415	10.152666
8.148301	671.363821	10.157683
8.493505	660.822154	10.162701
8.106750	666.203994	10.167719
8.274795	663.078184	10.172736
8.359572	673.937288	10.177754
8.559391	676.528871	10.182771
8.879577	676.488096	10.187789
8.683921	683.287612	10.192807
8.751840	671.886007	10.197824
8.386605	680.353652	10.202842
7.853310	672.253361	10.207859
8.509815	688.156050	10.212877
8.477335	688.012265	10.217895
8.599389	697.524945	10.222912
8.814524	703.361821	10.227930
8.643985	714.172882	10.232947
8.573770	704.279662	10.237965
8.906473	707.581877	10.242983
8.805723	701.566700	10.248000
8.589808	706.556114	10.253018
8.860535	710.066611	10.258035
9.016641	700.173318	10.263053
8.738267	712.157278	10.268071
8.992910	705.617924	10.273088
9.008577	709.966669	10.278106
8.810400	704.332954	10.283123
9.080107	697.598602	10.288141
8.648781	710.275562	10.293159
8.823240	702.851119	10.298176
8.870940	704.875020	10.303194
8.839291	705.384205	10.308211
9.070685	692.641622	10.313229
8.767762	686.687879	10.318247
8.883422	665.732930	10.323264
8.663805	682.386554	10.328282
8.742465	690.403757	10.333299
8.924165	691.767320	10.338317
8.599633	703.574283	10.343335
8.952532	709.102146	10.348352
9.111960	695.770335	10.353370
8.609904	706.302842	10.358387
8.971380	700.747312	10.363405
8.863464	706.546349	10.368423
9.000646	699.830792	10.373440
8.936641	700.924431	10.378458
8.751717	709.310467	10.383475
9.286748	700.526795	10.388493
9.044115	701.061074	10.393511
9.169381	704.433068	10.398528
9.046504	682.227718	10.403546
8.697818	675.179856	10.408563
8.892350	695.342635	10.413581
8.932285	697.340657	10.418599
8.969751	700.211474	10.423616
8.889501	702.015633	10.428634
8.859351	706.310156	10.433651
9.118533	693.213387	10.438669
8.963544	708.189712	10.443687
8.632182	702.938658	10.448704
8.906295	701.000122	10.453722
8.699939	702.978302	10.458739
8.951976	700.069467	10.463757
8.677537	700.355092	10.468775
8.690557	702.340250	10.473792
8.895035	701.378931	10.478810
8.789732	712.459879	10.483827
9.011899	714.335608	10.488845
9.231612	728.852688	10.493863
9.249888	725.742413	10.498880
9.140195	735.826136	10.503898
9.171324	740.650646	10.508915
9.151686	724.873808	10.513933
9.087651	731.747805	10.518951
9.125173	723.061461	10.523968
9.628275	729.193949	10.528986
9.108617	712.217324	10.534003
8.830296	703.404956	10.539021
8.737866	714.421966	10.544039
8.824272	728.231244	10.549056
9.218821	732.160979	10.554074
9.349731	734.631314	10.559091
9.201617	730.585658	10.564109
9.323795	732.581483	10.569127
9.150522	732.236222	10.574144
9.214512	727.426356	10.579162
9.371652	731.263522	10.584179
9.480561	735.836976	10.589197
9.198067	734.621666	10.594215
9.243215	736.369634	10.599232
9.358133	728.331848	10.604250
8.871979	724.011874	10.609267
9.277832	721.013002	10.614285
9.169644	725.629489	10.619303
9.347306	732.791790	10.624320
9.399614	726.241053	10.629338
9.449424	734.310298	10.634355
9.333775	733.978721	10.639373
9.222419	732.242190	10.644391
9.072596	730.466362	10.649408
9.606510	727.839567	10.654426
9.133338	730.300487	10.659443
9.171564	723.414703	10.664461
9.379180	731.721578	10.669479
9.329360	731.399179	10.674496
9.229294	727.853016	10.679514
9.241433	747.745100	10.684531
9.538115	745.075699	10.689549
9.764237	735.542814	10.694567
9.503759	735.706844	10.699584
9.572898	725.962966	10.704602
9.439434	731.908360	10.709619
9.525721	730.600885	10.714637
9.167705	731.951072	10.719655
9.639596	735.020809	10.724672
9.616516	724.459183	10.729690
9.353689	722.763875	10.734707
9.437157	734.014749	10.739725
9.396265	740.561709	10.744743
9.379620	748.932105	10.749760
9.911568	755.977488	10.754778
9.685637	745.227403	10.759795
9.619739	735.164955	10.764813
9.480117	737.374200	10.769831
8.973998	736.534481	10.774848
9.678014	746.427175	10.779866
9.623369	766.163028	10.784883
10.226026	757.220103	10.789901
9.799364	757.090805	10.794919
9.748639	747.622651	10.799936
9.433873	729.653870	10.804954
9.159431	737.590205	10.809971
9.778049	753.859254	10.814989
9.913403	760.431365	10.820007
9.486036	749.261511	10.825024
9.704548	746.477109	10.830042
9.905734	758.154150	10.835059
9.489304	743.159884	10.840077
9.689092	748.031267	10.845095
9.511026	768.333983	10.850112
9.834777	771.180241	10.855130
9.873094	776.904306	10.860147
9.958494	768.973743	10.865165
9.810546	749.060108	10.870183
9.540301	742.989127	10.875200
9.888740	738.387259	10.880218
9.676683	753.144745	10.885235
10.197554	750.840558	10.890253
9.900136	739.091352	10.895271
9.757643	735.134129	10.900288
9.904152	730.859777	10.905306
9.684200	742.600243	10.910323
9.758361	727.159424	10.915341
9.727765	729.261644	10.920359
9.643252	734.018298	10.925376
10.327649	735.717103	10.930394
9.660436	739.615581	10.935411
9.532476	728.618197	10.940429
9.791607	748.106019	10.945447
9.888079	763.873779	10.950464
10.265232	761.977618	10.955482
10.137103	762.069736	10.960499
10.060670	736.100543	10.965517
10.294203	732.549136	10.970535
9.892481	736.380031	10.975552
9.856352	729.654578	10.980570
9.771108	727.233451	10.985587
9.629572	728.518660	10.990605
10.104040	740.751580	10.995623
9.818003	760.836352	11.000640
10.046826	761.553181	11.005658
9.756015	761.464375	11.010675
10.077443	767.194703	11.015693
10.331022	758.128096	11.020711
10.032924	764.936147	11.025728
10.323568	761.537079	11.030746
10.006479	741.987660	11.035763
9.882613	732.752086	11.040781
10.043499	734.102565	11.045799
9.991078	762.897726	11.050816
10.499840	769.700512	11.055834
9.770600	743.607528	11.060851
9.952190	759.798958	11.065869
10.234272	760.130218	11.070887
10.154090	768.204864	11.075904
10.369757	755.710489	11.080922
10.228415	761.480438	11.085939
10.008402	741.763379	11.090957
10.113032	748.039410	11.095975
10.189385	765.289941	11.100992
10.317717	759.555686	11.106010
9.977938	755.899220	11.111027
10.161132	753.087990	11.116045
10.405009	762.865167	11.121063
10.118884	753.444650	11.126080
10.360453	752.697251	11.131098
10.592255	754.955225	11.136115
9.781585	740.379765	11.141133
9.894236	744.699862	11.146151
10.218649	758.654784	11.151168
10.181612	759.042035	11.156186
10.376211	762.215565	11.161203
10.196173	756.185150	11.166221
10.225023	759.044414	11.171239
10.018450	758.479876	11.176256
10.535951	757.141543	11.181274
10.037348	755.744706	11.186291
10.462056	759.874561	11.191309
10.267280	752.909636	11.196327
9.737948	763.654560	11.201344
9.935264	755.062204	11.206362
10.115648	763.838932	11.211379
9.953230	758.199670	11.216397
10.292443	760.884714	11.221415
10.204948	771.754500	11.226432
10.392536	775.671276	11.231450
10.494508	779.281775	11.236467
10.481395	778.158462	11.241485
10.573258	782.106443	11.246503
10.349527	782.363595	11.251520
10.724551	775.726331	11.256538
10.383898	782.635526	11.261555
10.586737	779.379332	11.266573
10.817752	779.963129	11.271591
10.489101	781.433647	11.276608
10.613524	773.337575	11.281626
10.537061	777.051632	11.286643
10.605711	779.841320	11.291661
10.668280	765.073998	11.296679
10.594339	764.648118	11.301696
10.715345	758.859174	11.306714
10.575418	752.606777	11.311731
10.374557	755.817444	11.316749
10.660967	753.096991	11.321767
10.404323	753.505253	11.326784
10.823149	753.482788	11.331802
10.436010	768.041733	11.336819
10.415439	768.975439	11.341837
10.800262	763.108952	11.346855
10.795614	771.149047	11.351872
10.509273	766.197585	11.356890
10.520567	780.679150	11.361907
10.704236	771.730798	11.366925
10.799423	771.599728	11.371943
10.532215	777.496818	11.376960
10.685455	771.629702	11.381978
10.765527	772.410136	11.386995
10.786088	775.079841	11.392013
10.684616	775.575001	11.397031
10.978417	781.417777	11.402048
10.891095	775.133433	11.407066
10.858777	771.874844	11.412083
10.826258	776.889815	11.417101
10.818758	778.097324	11.422119
10.678678	778.767765	11.427136
10.671507	776.607308	11.432154
10.653283	782.590329	11.437171
10.557148	782.329926	11.442189
10.632434	782.074993	11.447207
10.707094	784.363716	11.452224
10.879345	772.319010	11.457242
10.942522	774.477358	11.462259
10.577786	780.587437	11.467277
11.285158	775.526934	11.472295
10.593365	784.155593	11.477312
10.693721	774.599811	11.482330
11.069360	782.966288	11.487347
10.518037	779.860169	11.492365
11.025537	771.686886	11.497383
10.541425	775.101930	11.502400
10.961542	778.861312	11.507418
10.890620	778.321947	11.512435
10.556753	779.729159	11.517453
10.944391	786.487447	11.522471
10.873545	803.362417	11.527488
11.046800	809.238550	11.532506
11.174046	808.019162	11.537523
10.898202	811.702072	11.542541
11.250780	805.293697	11.547559
11.232037	808.557678	11.552576
10.943819	783.821831	11.557594
10.759635	784.390526	11.562611
10.989827	801.199899	11.567629
11.273664	815.448190	11.572647
11.034901	816.170010	11.577664
10.847561	802.079825	11.582682
11.136681	800.673800	11.587699
11.052853	806.940906	11.592717
11.129193	800.310967	11.597735
11.074869	802.986778	11.602752
11.136269	800.509075	11.607770
11.149122	804.658717	11.612787
11.102650	810.418093	11.617805
11.421688	803.837722	11.622823
11.114469	806.298338	11.627840
11.081858	806.989565	11.632858
11.532653	806.336645	11.637875
11.226752	803.613087	11.642893
11.323798	805.444983	11.647911
11.442196	809.347241	11.652928
11.429907	808.567864	11.657946
11.403316	803.644634	11.662963
11.490294	811.808546	11.667981
11.292019	806.636595	11.672999
11.331020	801.764706	11.678016
11.460629	806.208383	11.683034
11.517229	783.274782	11.688051
11.088096	789.433715	11.693069
11.296359	783.697632	11.698087
11.318983	805.232446	11.703104
11.158389	803.840655	11.708122
11.316023	798.009019	11.713139
11.231083	811.699509	11.718157
11.117754	803.707352	11.723175
11.164438	803.447313	11.728192
11.175825	819.699271	11.733210
11.651610	811.776480	11.738227
11.215929	805.228960	11.743245
11.102905	803.467896	11.748263
11.622828	810.893226	11.753280
11.212881	800.093657	11.758298
11.386294	803.180945	11.763315
11.266383	811.215738	11.768333
11.183518	798.177881	11.773351
11.367947	814.532275	11.778368
11.813951	832.611385	11.783386
11.539168	820.026526	11.788403
11.515190	822.297731	11.793421
11.630600	825.626899	11.798439
11.298102	822.088495	11.803456
11.795596	835.454228	11.808474
11.796883	824.622765	11.813491
11.630724	830.705494	11.818509
12.062748	811.327597	11.823527
11.763093	809.017546	11.828544
11.574779	807.875606	11.833562
11.396425	809.808614	11.838579
11.516430	817.011209	11.843597
11.611228	811.097459	11.848615
11.603696	811.396760	11.853632
11.614079	818.014391	11.858650
11.750468	810.272597	11.863667
11.637707	816.398444	11.868685
11.799893	828.848882	11.873703
11.560530	832.071845	11.878720
11.248132	841.103828	11.883738
11.762556	833.915533	11.888755
11.680407	837.002628	11.893773
11.359515	832.452513	11.898791
11.375372	838.744462	11.903808
11.684683	841.485257	11.908826
11.810547	839.491728	11.913843
11.312219	836.396899	11.918861
11.641125	834.624461	11.923879
11.845392	838.131032	11.928896
11.637500	850.398687	11.933914
12.168735	850.250134	11.938931
11.594558	854.675331	11.943949
12.276451	847.113648	11.948967
12.305433	839.892353	11.953984
11.505114	832.885150	11.959002
12.100782	830.400073	11.964019
11.915587	828.674576	11.969037
11.892908	830.890060	11.974055
12.244054	822.831218	11.979072
11.855781	844.840008	11.984090
12.033882	829.032684	11.989107
11.643120	830.593015	11.994125
11.942955	832.394090	11.999143
12.152587	844.982740	12.004160
11.978007	840.877268	12.009178
12.082067	836.863839	12.014195
11.931498	840.041000	12.019213
12.498566	840.415618	12.024231
12.226794	832.509129	12.029248
11.949316	830.697344	12.034266
12.196932	826.208597	12.039283
11.902223	827.877425	12.044301
12.326091	823.408309	12.049319
12.151432	827.708686	12.054336
11.860506	829.065094	12.059354
12.125561	833.846567	12.064371
12.329777	838.387736	12.069389
12.159997	823.503328	12.074407
11.865505	831.217847	12.079424
12.080006	846.945283	12.084442
12.354545	853.294004	12.089459
12.311113	864.006174	12.094477
12.283182	847.408581	12.099495
12.073651	850.048687	12.104512
12.146150	859.117335	12.109530
12.315875	852.177437	12.114547
12.293934	862.516381	12.119565
12.323106	863.931987	12.124583
12.750452	854.832219	12.129600
12.270866	847.876225	12.134618
12.292115	831.339401	12.139635
12.257908	835.405510	12.144653
12.003185	830.031098	12.149671
12.219427	840.889219	12.154688
12.559929	859.794842	12.159706
12.578920	856.238777	12.164723
12.427059	857.865845	12.169741
12.370062	852.801186	12.174759
12.724885	844.589764	12.179776
12.217285	840.879574	12.184794
12.499395	833.525034	12.189811
12.126490	832.886860	12.194829
12.465834	849.083363	12.199847
12.810342	854.589835	12.204864
12.365566	850.662164	12.209882
12.496169	840.216342	12.214899
12.318094	844.592481	12.219917
12.531854	868.136173	12.224935
12.622605	862.617147	12.229952
12.636302	854.654321	12.234970
12.563249	855.430983	12.239987
12.351956	853.728308	12.245005
12.606903	845.782623	12.250023
12.318457	856.444811	12.255040
12.474041	863.282500	12.260058
12.513480	855.834282	12.265075
12.670621	859.994296	12.270093
12.283928	870.684574	12.275111
12.958518	862.719390	12.280128
12.484913	857.536323	12.285146
12.604334	855.426148	12.290163
12.721264	859.003877	12.295181
12.663920	862.112458	12.300199
12.670009	856.433841	12.305216
12.349070	872.986146	12.310234
12.688699	860.706580	12.315251
12.499698	865.384124	12.320269
12.630965	869.546458	12.325287
12.680581	856.877145	12.330304
12.399827	866.084208	12.335322
12.622490	860.841749	12.340339
12.799251	877.343141	12.345357
12.820642	883.218071	12.350375
12.729211	881.563259	12.355392
12.740411	898.417267	12.360410
12.982388	885.583015	12.365427
13.044939	888.054064	12.370445
13.198321	882.612845	12.375463
13.069017	859.941792	12.380480
12.999153	852.381366	12.385498
12.882341	855.720254	12.390515
12.613319	860.216569	12.395533
12.859384	853.298674	12.400551
13.172981	856.879267	12.405568
12.554996	862.661648	12.410586
12.784687	876.091445	12.415603
12.890028	887.665957	12.420621
12.891938	887.682215	12.425639
12.998399	882.582606	12.430656
13.291959	884.653217	12.435674
12.919856	885.026273	12.440691
13.075198	889.682237	12.445709
13.118266	890.440460	12.450727
13.213415	892.280948	12.455744
13.360934	886.480086	12.460762
12.960224	876.337955	12.465779
13.121751	867.479824	12.470797
13.047849	870.817121	12.475815
12.905687	871.133598	12.480832
12.875801	879.170054	12.485850
13.200630	882.942091	12.490867
13.235335	891.272960	12.495885
12.730836	895.609863	12.500903
13.018126	889.012668	12.505920
13.373490	890.501815	12.510938
13.119309	884.939509	12.515955
13.018889	897.542536	12.520973
13.096709	893.770040	12.525991
13.028366	890.915795	12.531008
13.272443	888.285789	12.536026
13.244208	899.876129	12.541043
12.949606	890.225842	12.546061
13.284599	894.214297	12.551079
13.403399	892.408536	12.556096
13.083051	907.425426	12.561114
13.389070	906.235480	12.566131
13.478735	900.769374	12.571149
13.310959	895.596279	12.576167
13.725077	889.969764	12.581184
13.278328	891.578345	12.586202
13.188949	888.727191	12.591219
13.146377	889.850757	12.596237
13.483982	886.058473	12.601255
13.491643	891.384134	12.606272
13.227801	892.492768	12.611290
13.056569	891.599555	12.616307
13.047734	900.883653	12.621325
13.218105	914.639038	12.626343
13.598903	910.417176	12.631360
13.684789	924.062943	12.636378
13.758445	924.368487	12.641395
13.602122	918.094330	12.646413
13.633144	918.300639	12.651431
13.896425	918.763750	12.656448
13.731126	921.310327	12.661466
14.037135	914.080526	12.666483
13.877746	889.506239	12.671501
13.575970	884.030156	12.676519
13.857387	889.522680	12.681536
13.447724	890.074388	12.686554
13.582104	878.049650	12.691571
13.719683	876.473839	12.696589
13.643068	881.054437	12.701607
13.896377	871.449254	12.706624
13.736220	874.170946	12.711642
13.723650	875.729678	12.716659
13.844917	874.010908	12.721677
13.356450	873.496193	12.726695
13.890764	881.117589	12.731712
13.516851	880.726024	12.736730
13.584882	881.906469	12.741747
13.912302	885.897751	12.746765
13.954590	897.079976	12.751783
13.736296	887.179271	12.756800
13.589435	888.240583	12.761818
13.908530	908.990267	12.766835
14.299501	902.105439	12.771853
13.876598	895.307745	12.776871
14.114014	880.463726	12.781888
13.714917	877.115855	12.786906
13.541471	889.138479	12.791923
13.704459	889.221367	12.796941
13.753997	910.771948	12.801959
13.824448	912.426774	12.806976
13.952860	918.686732	12.811994
13.871569	917.603830	12.817011
14.486856	909.307909	12.822029
13.880231	914.124302	12.827047
14.070791	906.212868	12.832064
13.945300	913.458127	12.837082
13.794293	909.647537	12.842099
13.953266	911.033780	12.847117
13.856569	918.632917	12.852135
13.698949	914.324233	12.857152
14.183726	916.372240	12.862170
13.998165	919.341442	12.867187
14.121182	916.246067	12.872205
13.991833	910.852836	12.877223
13.970845	912.098808	12.882240
13.990507	917.088255	12.887258
13.745843	913.997468	12.892275
14.123237	909.517127	12.897293
13.876647	913.168054	12.902311
14.283709	925.883519	12.907328
14.277593	935.829754	12.912346
14.135332	940.756655	12.917363
14.746586	934.110521	12.922381
14.406843	925.925095	12.927399
14.355113	921.801621	12.932416
14.388465	913.378053	12.937434
14.174011	918.055891	12.942451
14.226581	912.703398	12.947469
14.274960	911.151015	12.952487
14.393835	902.540466	12.957504
14.232629	901.433792	12.962522
14.360432	913.715592	12.967539
14.363944	921.822126	12.972557
14.236807	933.791056	12.977575
14.629959	935.714874	12.982592
13.998250	937.423375	12.987610
13.765267	944.680149	12.992627
14.527959	934.221720	12.997645
14.242264	948.040449	13.002663
14.415248	940.628341	13.007680
14.677130	943.849819	13.012698
14.465921	943.928137	13.017715
14.960925	941.958506	13.022733
14.555099	937.967673	13.027751
14.535063	943.189676	13.032768
14.775281	938.443079	13.037786
14.901338	934.248039	13.042803
14.776948	930.582241	13.047821
14.352337	940.393849	13.052839
14.657834	939.042578	13.057856
14.694002	935.914339	13.062874
14.679000	938.926559	13.067891
14.860585	935.374260	13.072909
14.656428	936.877325	13.077927
14.734823	932.871664	13.082944
14.843169	931.929399	13.087962
14.600022	934.505009	13.092979
15.080352	932.778742	13.097997
14.938871	943.852067	13.103015
14.744363	936.154767	13.108032
14.994985	930.304929	13.113050
14.515280	925.749589	13.118067
14.920540	923.031866	13.123085
14.906260	934.193171	13.128103
14.861535	929.972870	13.133120
14.740934	921.203943	13.138138
14.825427	929.630520	13.143155
14.933199	920.633629	13.148173
14.596145	923.031884	13.153191
14.674318	930.835523	13.158208
14.896561	933.245493	13.163226
14.854818	931.837159	13.168243
14.984723	935.199382	13.173261
14.870340	934.536898	13.178279
14.901072	937.413992	13.183296
14.811396	937.560764	13.188314
14.800017	935.721045	13.193331
14.868134	927.527922	13.198349
14.725032	935.960301	13.203367
14.979208	939.703502	13.208384
15.180248	932.489892	13.213402
14.996955	940.624219	13.218419
15.058101	930.884292	13.223437
15.226571	933.817314	13.228455
14.811584	930.001613	13.233472
14.834396	930.855708	13.238490
14.955357	934.065087	13.243507
15.051423	934.200000	13.248525
15.081971	942.453636	13.253543
15.192886	956.422043	13.258560
15.346270	964.047505	13.263578
15.218542	956.196624	13.268595
15.333449	945.949777	13.273613
15.097865	946.307708	13.278631
15.268319	954.840532	13.283648
15.425564	953.429954	13.288666
15.416718	941.696587	13.293683
15.313925	934.627770	13.298701
15.349410	932.534634	13.303719
15.535598	937.944130	13.308736
15.329542	932.443913	13.313754
15.213027	942.659601	13.318771
15.330382	930.617564	13.323789
15.293120	937.716734	13.328807
15.180061	948.114916	13.333824
15.308078	956.250457	13.338842
15.475565	966.728175	13.343859
15.783427	955.421860	13.348877
15.711684	962.179918	13.353895
15.503953	951.250699	13.358912
15.289610	933.129232	13.363930
15.514327	944.220656	13.368947
15.360042	960.033681	13.373965
15.612895	962.278359	13.378983
15.830524	964.669413	13.384000
15.988135	947.086311	13.389018
15.404002	940.445210	13.394035
15.458474	939.859092	13.399053
15.248043	941.945452	13.404071
15.473735	955.702736	13.409088
15.731045	962.348043	13.414106
15.748262	967.535933	13.419123
15.859844	965.833717	13.424141
15.494012	961.479185	13.429159
15.644772	967.024079	13.434176
15.678006	971.209759	13.439194
15.580739	979.034206	13.444211
15.511742	967.927286	13.449229
15.690840	964.000214	13.454247
15.484468	967.903142	13.459264
15.668116	969.512854	13.464282
15.650395	968.676890	13.469299
16.102586	971.026350	13.474317
15.659610	963.722131	13.479335
15.689482	967.583578	13.484352
15.674433	965.568487	13.489370
15.463974	964.827428	13.494387
15.496244	968.242043	13.499405
15.432059	975.340571	13.504423
15.566179	988.889437	13.509440
16.038549	987.115666	13.514458
15.945305	996.492535	13.519475
16.339614	990.295274	13.524493
16.080917	993.799411	13.529511
16.134783	994.452707	13.534528
16.481650	986.196860	13.539546
16.312523	981.790067	13.544563
16.207407	964.217774	13.549581
16.054826	960.875126	13.554599
16.044938	966.337964	13.559616
16.178416	953.132270	13.564634
15.863648	961.918664	13.569651
16.192910	950.376930	13.574669
16.187221	957.445293	13.579687
15.985111	957.757526	13.584704
16.417028	949.076218	13.589722
16.332314	961.145620	13.594739
16.622635	949.009970	13.599757
16.530380	955.293097	13.604775
16.419425	958.678673	13.609792
16.551107	951.380875	13.614810
16.031507	953.087348	13.619827
16.505339	954.200997	13.624845
16.764369	963.342357	13.629863
16.361631	960.084831	13.634880
16.766692	949.707263	13.639898
16.372467	944.067735	13.644915
16.388271	929.087932	13.649933
16.128430	929.864820	13.654951
16.144191	935.666297	13.659968
16.564556	947.356793	13.664986
16.376830	953.283305	13.670003
16.404870	950.997314	13.675021
16.208829	952.629739	13.680039
16.157896	958.453291	13.685056
16.382726	945.790718	13.690074
16.221922	956.820010	13.695091
16.335252	955.019872	13.700109
16.337363	956.643894	13.705127
16.088397	952.097975	13.710144
15.981188	952.038211	13.715162
16.038084	961.485075	13.720179
16.311687	973.403820	13.725197
16.680685	982.928539	13.730215
16.604800	983.532456	13.735232
16.993752	982.266176	13.740250
16.502717	989.133437	13.745267
16.184135	992.223493	13.750285
16.736357	988.342893	13.755303
16.384353	993.947033	13.760320
16.313992	988.731006	13.765338
16.455379	984.575931	13.770355
16.300282	985.046908	13.775373
16.824587	996.374969	13.780391
16.755025	1009.070217	13.785408
16.984402	1007.048898	13.790426
16.616646	1001.141986	13.795443
16.846386	1003.032638	13.800461
16.958218	1008.920593	13.805479
16.932809	1010.490519	13.810496
16.924772	989.883356	13.815514
16.765209	990.744425	13.820531
16.898158	992.364108	13.825549
16.817159	996.891531	13.830567
16.821949	1008.161144	13.835584
17.142544	1002.742980	13.840602
17.058242	1015.461933	13.845619
16.822884	1001.132284	13.850637
17.218612	997.567739	13.855655
16.845980	1004.785857	13.860672
17.190528	999.089724	13.865690
16.841659	1006.634995	13.870707
17.388360	1000.925465	13.875725
16.989497	991.474653	13.880743
16.757148	998.082163	13.885760
17.152929	1001.448798	13.890778
16.965762	1010.670369	13.895795
17.043240	1005.188135	13.900813
17.290456	1002.591053	13.905831
17.086109	1009.795873	13.910848
17.060928	1001.140227	13.915866
17.176537	1007.998379	13.920883
17.213385	1002.565391	13.925901
17.597234	1000.427947	13.930919
17.391231	1006.955117	13.935936
17.382400	1008.903384	13.940954
17.522803	1003.692214	13.945971
17.392519	1010.547384	13.950989
17.638616	1000.084298	13.956007
16.991461	994.903151	13.961024
17.594762	998.091728	13.966042
17.505905	995.401483	13.971059
17.460258	983.973377	13.976077
17.404103	984.322463	13.981095
17.515174	985.945768	13.986112
17.221009	973.708465	13.991130
17.373606	983.485937	13.996147
17.309409	996.019270	14.001165
17.416986	1002.937408	14.006183
17.443204	1010.423721	14.011200
17.670027	1004.304580	14.016218
17.568944	1015.040178	14.021235
17.516007	1008.600840	14.026253
17.845069	1000.237310	14.031271
17.733910	1012.852838	14.036288
17.628270	1006.270660	14.041306
17.598764	1000.343957	14.046323
17.476973	1004.848611	14.051341
18.149000	992.829241	14.056359
17.367638	990.520583	14.061376
17.189796	991.349641	14.066394
17.377426	1002.545669	14.071411
17.407456	998.837357	14.076429
17.386430	996.635465	14.081447
17.302287	999.233968	14.086464
17.477284	1011.403704	14.091482
17.542570	1011.008305	14.096499
17.620472	1019.543498	14.101517
18.180300	1028.366991	14.106535
17.956302	1036.661252	14.111552
17.947645	1023.367621	14.116570
17.851366	1026.824006	14.121587
17.819265	1030.884306	14.126605
18.256153	1020.733301	14.131623
17.826506	1016.490891	14.136640
18.213028	1009.985870	14.141658
18.137429	997.726135	14.146675
17.934351	1001.413576	14.151693
17.843685	994.134465	14.156711
17.541557	999.699247	14.161728
17.796754	1006.045329	14.166746
17.862952	1023.391133	14.171763
17.823872	1019.222232	14.176781
18.156578	1026.053105	14.181799
18.069322	1026.673472	14.186816
18.038572	1025.499913	14.191834
18.384432	1026.743415	14.196851
18.016923	1032.889089	14.201869
18.816212	1022.783582	14.206887
18.360831	1029.163480	14.211904
18.193608	1029.837245	14.216922
18.113833	1026.135298	14.221939
17.957410	1032.118465	14.226957
18.207410	1028.491040	14.231975
18.153115	1028.253230	14.236992
18.017040	1024.759023	14.242010
18.246342	1020.622844	14.247027
18.032449	1029.540991	14.252045
18.144929	1023.932094	14.257063
18.493704	1029.045026	14.262080
18.281345	1024.483968	14.267098
18.646638	1017.956870	14.272115
18.160599	1030.314029	14.277133
18.698630	1016.711779	14.282151
18.487025	1028.855786	14.287168
18.430827	1021.301281	14.292186
18.905834	1022.237977	14.297203
18.792467	1023.220527	14.302221
18.868589	1015.331136	14.307239
18.755315	1020.952446	14.312256
18.782086	1018.358400	14.317274
18.913406	1015.117149	14.322291
18.505578	1013.508414	14.327309
18.315067	1009.309869	14.332327
18.496694	1023.865028	14.337344
18.561869	1020.133176	14.342362
18.674478	1020.383848	14.347379
18.558221	1026.061950	14.352397
18.307019	1022.030531	14.357415
18.526735	1029.551346	14.362432
18.464390	1020.474697	14.367450
18.515448	1023.789367	14.372467
18.555392	1032.151333	14.377485
18.790661	1023.437195	14.382503
18.850443	1023.094672	14.387520
18.416536	1028.810020	14.392538
18.640976	1040.646410	14.397555
18.581773	1052.623866	14.402573
18.734025	1050.177535	14.407591
18.864571	1052.572394	14.412608
18.764242	1055.151933	14.417626
18.738402	1059.924955	14.422643
18.569067	1059.973505	14.427661
18.966286	1050.331784	14.432679
18.704711	1059.465316	14.437696
18.954182	1060.468099	14.442714
19.214902	1061.636729	14.447731
18.907276	1057.361504	14.452749
19.159995	1053.123806	14.457767
19.050600	1048.404359	14.462784
18.855069	1054.042450	14.467802
18.777784	1053.896632	14.472819
18.949343	1060.442405	14.477837
19.377197	1075.457608	14.482855
19.412536	1082.510967	14.487872
19.052669	1069.104592	14.492890
19.164858	1058.199486	14.497907
19.402648	1064.790591	14.502925
19.401822	1052.379461	14.507943
19.259224	1048.567444	14.512960
19.008586	1047.185422	14.517978
19.255792	1055.763071	14.522995
19.581671	1071.986446	14.528013
19.727131	1061.028586	14.533031
19.602587	1050.259532	14.538048
19.319649	1047.778573	14.543066
19.578110	1037.073268	14.548083
19.258189	1046.644782	14.553101
19.189650	1044.721605	14.558119
19.270015	1048.888872	14.563136
19.094295	1048.411730	14.568154
19.494005	1057.626305	14.573171
19.544525	1067.173892	14.578189
19.889063	1061.501753	14.583207
19.834931	1049.542347	14.588224
19.654585	1044.917717	14.593242
19.827855	1049.510528	14.598259
19.587081	1043.380219	14.603277
19.612833	1042.649647	14.608295
19.787580	1046.278473	14.613312
19.628212	1036.322641	14.618330
19.700200	1043.303774	14.623347
19.309586	1042.062643	14.628365
19.869099	1042.129477	14.633383
19.746577	1042.319876	14.638400
19.678840	1043.006300	14.643418
19.795100	1037.088123	14.648435
19.423084	1041.132667	14.653453
19.314003	1047.731203	14.658471
19.230737	1057.604468	14.663488
20.057875	1071.285493	14.668506
20.199279	1063.923436	14.673523
20.138709	1062.673319	14.678541
20.060357	1064.781524	14.683559
20.069614	1067.689362	14.688576
20.163513	1067.604565	14.693594
20.389086	1050.319922	14.698611
19.752498	1041.221816	14.703629
20.045322	1038.369942	14.708647
20.025293	1038.799264	14.713664
19.982333	1037.321440	14.718682
20.348006	1033.728795	14.723699
19.862109	1037.896915	14.728717
20.012256	1035.135199	14.733735
20.380341	1032.668485	14.738752
20.044830	1043.231513	14.743770
19.994325	1038.524364	14.748787
19.870072	1039.744141	14.753805
19.977256	1048.534727	14.758823
20.312525	1066.149791	14.763840
20.023447	1068.826725	14.768858
20.082112	1061.891739	14.773875
20.115818	1068.869381	14.778893
20.340414	1060.394381	14.783911
20.456385	1060.333093	14.788928
20.035973	1066.947758	14.793946
20.070122	1051.901809	14.798963
19.951665	1057.725163	14.803981
20.163230	1055.288693	14.808999
20.180805	1058.022719	14.814016
19.988367	1065.027175	14.819034
20.577843	1072.925350	14.824051
20.744224	1092.417548	14.829069
20.550980	1076.738781	14.834087
20.876550	1062.838613	14.839104
20.518085	1065.151461	14.844122
20.810674	1061.702009	14.849139
19.865074	1059.943742	14.854157
20.425505	1053.842172	14.859175
20.557031	1071.327600	14.864192
20.441955	1089.237330	14.869210
20.870935	1091.079255	14.874227
20.816062	1092.033620	14.879245
20.735728	1079.615161	14.884263
21.142525	1069.173056	14.889280
20.610724	1066.715192	14.894298
20.761163	1058.731981	14.899315
20.643811	1061.924158	14.904333
20.384556	1053.197405	14.909351
20.688554	1075.168267	14.914368
20.744137	1087.564128	14.919386
21.047462	1089.520163	14.924403
20.925796	1089.687193	14.929421
20.841184	1090.762225	14.934439
21.219514	1087.118262	14.939456
20.978149	1086.343338	14.944474
21.171826	1071.491812	14.949491
20.997148	1061.147177	14.954509
21.011512	1065.878505	14.959527
21.168284	1053.079875	14.964544
20.728068	1057.509323	14.969562
21.220793	1044.996396	14.974579
20.840008	1059.772663	14.979597
20.849599	1060.899809	14.984615
21.257820	1074.116366	14.989632
20.963006	1091.219280	14.994650
21.263238	1084.158066	14.999667
20.943888	1088.079732	15.004685
21.073661	1088.779121	15.009703
21.194520	1090.555142	15.014720
20.847382	1096.740773	15.019738
21.116815	1086.943424	15.024755
21.067453	1084.010020	15.029773
21.347888	1085.272234	15.034791
21.317875	1088.717267	15.039808
20.986079	1084.724372	15.044826
21.249867	1080.293502	15.049843
21.123244	1084.146248	15.054861
21.154658	1080.892788	15.059879
21.295152	1088.296046	15.064896
21.257159	1092.358913	15.069914
21.555144	1098.263319	15.074931
21.421230	1096.590322	15.079949
21.207140	1114.407819	15.084967
21.770509	1108.642737	15.089984
21.477424	1110.375496	15.095002
21.665407	1109.249961	15.100019
21.681792	1108.051663	15.105037
21.555677	1103.166077	15.110055
21.961666	1096.501503	15.115072
21.884792	1098.281527	15.120090
21.586615	1082.231562	15.125107
21.469528	1081.197881	15.130125
21.824622	1085.671228	15.135143
21.799226	1072.878338	15.140160
21.042365	1082.185624	15.145178
21.787204	1087.034576	15.150195
21.837144	1104.474104	15.155213
21.914146	1106.726662	15.160231
22.147282	1103.164609	15.165248
21.870763	1106.567789	15.170266
22.068840	1095.568910	15.175283
21.909634	1096.519292	15.180301
21.756779	1093.267209	15.185319
21.888839	1096.238573	15.190336
22.084679	1105.839284	15.195354
22.027948	1097.498246	15.200371
22.217318	1094.271775	15.205389
21.954502	1088.388790	15.210407
21.983291	1078.913172	15.215424
21.813844	1084.224920	15.220442
21.823654	1100.956944	15.225459
22.163421	1097.101655	15.230477
22.083850	1100.098221	15.235495
22.340256	1096.018162	15.240512
21.910313	1101.132902	15.245530
22.325841	1091.488912	15.250547
22.286892	1094.451586	15.255565
22.496018	1096.351175	15.260583
22.074250	1092.266488	15.265600
22.070257	1106.963087	15.270618
22.203959	1096.292572	15.275635
22.417733	1092.425470	15.280653
22.347667	1102.375315	15.285671
22.510717	1096.002928	15.290688
22.274570	1096.244031	15.295706
22.610728	1091.801961	15.300723
22.274613	1093.392637	15.305741
22.071985	1101.810554	15.310759
22.432638	1093.400800	15.315776
22.141658	1109.790921	15.320794
22.254930	1096.292005	15.325811
22.297173	1098.940854	15.330829
22.613477	1090.478605	15.335847
22.217591	1091.160315	15.340864
22.173574	1109.131134	15.345882
22.233044	1119.143395	15.350899
22.490321	1119.161461	15.355917
22.464556	1123.182155	15.360935
22.799401	1121.050054	15.365952
22.426060	1122.630361	15.370970
22.717460	1129.911017	15.375987
22.868728	1127.048316	15.381005
22.750293	1125.186539	15.386023
22.847879	1124.618865	15.391040
23.042435	1123.098947	15.396058
22.778674	1122.787163	15.401075
23.093187	1134.888228	15.406093
23.240337	1130.616810	15.411111
23.270946	1126.032812	15.416128
23.132295	1121.654790	15.421146
23.238618	1124.740260	15.426163
22.971270	1104.366033	15.431181
22.465223	1108.774900	15.436199
22.710345	1113.505040	15.441216
22.674746	1122.227188	15.446234
22.796289	1128.068700	15.451251
22.779014	1125.598854	15.456269
22.929455	1133.870928	15.461287
23.154282	1125.368691	15.466304
22.986122	1130.004676	15.471322
23.019480	1127.312674	15.476339
23.139625	1121.886324	15.481357
23.021603	1127.365943	15.486375
23.076860	1122.090095	15.491392
23.279442	1138.369388	15.496410
23.463102	1145.072243	15.501427
23.554986	1136.571541	15.506445
23.303564	1133.498757	15.511463
23.954024	1117.857402	15.516480
23.651040	1116.734820	15.521498
23.709912	1118.092777	15.526515
23.779129	1112.700845	15.531533
23.221641	1115.684821	15.536551
23.399316	1119.025788	15.541568
23.381775	1127.159932	15.546586
23.250534	1118.883974	15.551603
23.631604	1112.691219	15.556621
23.412642	1116.531311	15.561639
23.539618	1109.997969	15.566656
23.349216	1122.836150	15.571674
23.413777	1114.937206	15.576691
23.979457	1115.880547	15.581709
23.541998	1121.539432	15.586727
23.555696	1113.574898	15.591744
23.334889	1115.430724	15.596762
23.782849	1123.265352	15.601779
23.721877	1117.841829	15.606797
23.769889	1135.654532	15.611815
23.846606	1129.416501	15.616832
23.870584	1117.670085	15.621850
23.693201	1127.991640	15.626867
24.069860	1130.396544	15.631885
23.686349	1138.457045	15.636903
23.981730	1128.872689	15.641920
24.076646	1129.482580	15.646938
24.148582	1133.675675	15.651955
24.136741	1132.216703	15.656973
23.899312	1118.140035	15.661991
24.293360	1122.883705	15.667008
23.961170	1117.565325	15.672026
23.767105	1121.291457	15.677043
24.028249	1124.379243	15.682061
23.953459	1128.418292	15.687079
23.948158	1120.874602	15.692096
24.104489	1135.202173	15.697114
24.153778	1134.506674	15.702131
24.338322	1126.485499	15.707149
23.944968	1137.348709	15.712167
24.137227	1131.025013	15.717184
24.323330	1127.334526	15.722202
24.316828	1129.578474	15.727219
24.359088	1124.553194	15.732237
24.088512	1130.102168	15.737255
24.434851	1134.782878	15.742272
24.115342	1129.374995	15.747290
23.847247	1127.341156	15.752307
24.117726	1133.813102	15.757325
24.277842	1148.144390	15.762343
24.616622	1152.165750	15.767360
24.443814	1157.149351	15.772378
24.579754	1167.950923	15.777395
24.721867	1162.069361	15.782413
24.453314	1167.103463	15.787431
24.885050	1161.915652	15.792448
24.811211	1162.281449	15.797466
24.555439	1161.654178	15.802483
24.605074	1155.017485	15.807501
24.474789	1164.415549	15.812519
24.514564	1166.342008	15.817536
24.766659	1157.963186	15.822554
24.485988	1159.363985	15.827571
24.745562	1157.502207	15.832589
24.693720	1158.004515	15.837607
24.630587	1147.250026	15.842624
24.998466	1155.310522	15.847642
24.562854	1160.080169	15.852659
24.994534	1154.340026	15.857677
24.941239	1156.407481	15.862695
24.547607	1157.809268	15.867712
25.164376	1172.822811	15.872730
25.288326	1180.437901	15.877747
25.046543	1160.845561	15.882765
25.336701	1158.859038	15.887783
25.136015	1152.536227	15.892800
25.226845	1150.093752	15.897818
25.188306	1154.983075	15.902835
25.111679	1140.769527	15.907853
25.030822	1148.581106	15.912871
25.352327	1150.095178	15.917888
25.176265	1154.588783	15.922906
25.044458	1153.225656	15.927923
25.328271	1153.840489	15.932941
25.469844	1170.770447	15.937959
25.441416	1172.450335	15.942976
25.435941	1153.696405	15.947994
25.150635	1147.138797	15.953011
25.374943	1156.002174	15.958029
25.499268	1178.029311	15.963047
25.817209	1177.614905	15.968064
25.714217	1164.463147	15.973082
25.368260	1160.238726	15.978099
25.475030	1141.295365	15.983117
25.611895	1150.697609	15.988135
25.369894	1147.370908	15.993152
25.774256	1152.109336	15.998170
25.415270	1175.913290	16.003187
25.961825	1166.640852	16.008205
25.761050	1177.023397	16.013223
25.676678	1169.444746	16.018240
25.984187	1165.394002	16.023258
25.745881	1151.686333	16.028275
25.657167	1152.599062	16.033293
25.668844	1172.237446	16.038311
25.978169	1168.303719	16.043328
26.093852	1173.148221	16.048346
25.891598	1178.441025	16.053363
26.225361	1161.065118	16.058381
25.884098	1158.334752	16.063399
25.503929	1157.182823	16.068416
26.165055	1162.045268	16.073434
25.947478	1173.982116	16.078451
25.999987	1172.551854	16.083469
25.742697	1171.672087	16.088487
25.941220	1172.115616	16.093504
26.010690	1173.034436	16.098522
26.123174	1174.438244	16.103539
26.183973	1164.272257	16.108557
26.113720	1166.534640	16.113575
25.982626	1174.925005	16.118592
26.187058	1164.821846	16.123610
26.109872	1173.126907	16.128627
26.392622	1167.707079	16.133645
26.310162	1175.716569	16.138663
26.063044	1168.029045	16.143680
26.472251	1161.285567	16.148698
26.462644	1172.377769	16.153715
26.242955	1160.420889	16.158733
25.849972	1177.727154	16.163751
26.318169	1199.849739	16.168768
26.954295	1194.151711	16.173786
26.494991	1201.025620	16.178803
26.581410	1190.925843	16.183821
26.845857	1200.170775	16.188839
26.479394	1200.239762	16.193856
26.722692	1188.938457	16.198874
26.745882	1201.972037	16.203891
26.741052	1187.340272	16.208909
26.656193	1195.477330	16.213927
26.534241	1185.872281	16.218944
26.449166	1178.720500	16.223962
26.634809	1192.305500	16.228979
26.902161	1196.829629	16.233997
26.762944	1199.360909	16.239015
26.754763	1202.873216	16.244032
26.936809	1192.267856	16.249050
26.761024	1198.888131	16.254067
26.801642	1195.395729	16.259085
26.696220	1185.287172	16.264103
26.682335	1183.418311	16.269120
27.083006	1191.842283	16.274138
26.860323	1188.564735	16.279155
27.119100	1182.814630	16.284173
27.061809	1184.242613	16.289191
26.663316	1189.815151	16.294208
27.081959	1196.823991	16.299226
26.996436	1211.386162	16.304243
27.282600	1216.731172	16.309261
27.335119	1220.704678	16.314279
26.997697	1228.085960	16.319296
27.181981	1216.639293	16.324314
27.188470	1224.379362	16.329331
27.586154	1218.525144	16.334349
27.600928	1221.361627	16.339367
27.539891	1218.902163	16.344384
27.377743	1225.259963	16.349402
27.583546	1212.763310	16.354419
27.529660	1209.987712	16.359437
27.657296	1216.801447	16.364455
27.105444	1213.777211	16.369472
27.600058	1203.209849	16.374490
27.565598	1221.360706	16.379507
27.669219	1204.003569	16.384525
27.629324	1218.276704	16.389543
27.748216	1215.071721	16.394560
27.524635	1200.723007	16.399578
27.727700	1209.905670	16.404595
27.639582	1215.330370	16.409613
27.534182	1215.387231	16.414631
27.410730	1218.891071	16.419648
27.693221	1206.535263	16.424666
27.692252	1217.926452	16.429683
27.855854	1205.306876	16.434701
27.970536	1210.074391	16.439719
27.914347	1205.688595	16.444736
27.968936	1203.658399	16.449754
27.717481	1212.099814	16.454771
27.903106	1209.778243	16.459789
27.851041	1223.048311	16.464807
27.676275	1231.630971	16.469824
28.012105	1244.277002	16.474842
28.026033	1247.756919	16.479859
28.266481	1246.515210	16.484877
28.319254	1238.948855	16.489895
27.953876	1245.019851	16.494912
28.350935	1234.059184	16.499930
28.401706	1241.000615	16.504947
28.453677	1232.736777	16.509965
28.772502	1233.221410	16.514983
28.603098	1232.721957	16.520000
28.879520	1221.278533	16.525018
28.353117	1216.341872	16.530035
28.268043	1207.593276	16.535053
28.534440	1195.400767	16.540071
28.438038	1204.771986	16.545088
28.484926	1195.604314	16.550106
28.524656	1210.030393	16.555123
28.582714	1204.018643	16.560141
28.645369	1204.110273	16.565159
28.332257	1201.747274	16.570176
28.792489	1215.232104	16.575194
28.826107	1223.301529	16.580211
28.612245	1208.249645	16.585229
28.903883	1208.491543	16.590247
28.160871	1207.924083	16.595264
28.839550	1206.288170	16.600282
28.649316	1237.029808	16.605299
28.825477	1240.123422	16.610317
28.861338	1234.277930	16.615335
28.771714	1238.160019	16.620352
29.103371	1236.096145	16.625370
29.113723	1236.707445	16.630387
28.865542	1232.856567	16.635405
29.039076	1228.775235	16.640423
28.719774	1230.690295	16.645440
28.789072	1222.947201	16.650458
28.861247	1230.605139	16.655475
28.674713	1229.605781	16.660493
29.009642	1225.133564	16.665511
28.629052	1223.015192	16.670528
28.732693	1232.082840	16.675546
29.562173	1245.473485	16.680563
29.308823	1251.046027	16.685581
29.527985	1256.241520	16.690599
29.162681	1257.414221	16.695616
29.835434	1237.352644	16.700634
29.449504	1246.510420	16.705651
29.571410	1245.752499	16.710669
29.582125	1227.328860	16.715687
29.536915	1220.649578	16.720704
29.566731	1212.169741	16.725722
29.450057	1217.194459	16.730739
29.410690	1217.600217	16.735757
29.464461	1223.821480	16.740775
29.715159	1241.474370	16.745792
29.731401	1245.592074	16.750810
29.678904	1246.448026	16.755827
29.460698	1256.780757	16.760845
29.717287	1249.571976	16.765863
29.651979	1255.177160	16.770880
29.667831	1246.500016	16.775898
29.655077	1248.654074	16.780915
29.515929	1254.582894	16.785933
29.704455	1246.910987	16.790951
29.104469	1258.797838	16.795968
29.280165	1250.804835	16.800986
29.885217	1262.880727	16.806003
29.781063	1277.303135	16.811021
29.899641	1275.214304	16.816039
30.180760	1282.155799	16.821056
29.930017	1280.908021	16.826074
30.006645	1282.776819	16.831091
30.194283	1277.408528	16.836109
30.550389	1275.597287	16.841127
30.209376	1290.958903	16.846144
30.365636	1293.291670	16.851162
30.457472	1282.000810	16.856179
30.309209	1278.788870	16.861197
30.627149	1282.213732	16.866215
30.665593	1281.060192	16.871232
30.567482	1266.245377	16.876250
30.403208	1250.002597	16.881267
30.154658	1244.475052	16.886285
30.549055	1251.579661	16.891303
30.108633	1260.746074	16.896320
30.486026	1269.391654	16.901338
30.701288	1269.341090	16.906355
30.353495	1277.127644	16.911373
30.578498	1269.968571	16.916391
30.499496	1282.934103	16.921408
30.744289	1281.488528	16.926426
30.569138	1265.150291	16.931443
30.594071	1279.368654	16.936461
30.616605	1268.534937	16.941479
30.518661	1274.822679	16.946496
30.539544	1269.996556	16.951514
30.574270	1272.244721	16.956531
30.519263	1270.530293	16.961549
30.416513	1275.492883	16.966567
30.654403	1293.748725	16.971584
30.811236	1293.620436	16.976602
31.056314	1291.106336	16.981619
31.289287	1296.733009	16.986637
31.236562	1295.065837	16.991655
31.314830	1298.593772	16.996672
31.101710	1298.349974	17.001690
31.399072	1288.013242	17.006707
31.453574	1286.754289	17.011725
31.177335	1267.399402	17.016743
30.835277	1265.538416	17.021760
30.929732	1273.227331	17.026778
31.536197	1286.997058	17.031795
31.354021	1287.994560	17.036813
31.672073	1285.515621	17.041831
31.654861	1292.831708	17.046848
31.501681	1284.638425	17.051866
31.433189	1275.305564	17.056883
31.426726	1289.283079	17.061901
31.665731	1286.408971	17.066919
31.525264	1284.771682	17.071936
31.448199	1284.602597	17.076954
31.553144	1285.322248	17.081971
31.356701	1290.726330	17.086989
31.855744	1291.954727	17.092007
31.666082	1283.895435	17.097024
31.534747	1286.908876	17.102042
31.521747	1284.016655	17.107059
31.430621	1287.622241	17.112077
31.680398	1288.507669	17.117095
31.761912	1284.569904	17.122112
31.651151	1287.007905	17.127130
31.481375	1286.429773	17.132147
31.415484	1295.147980	17.137165
31.881406	1304.167887	17.142183
31.892425	1313.332413	17.147200
31.858092	1312.802717	17.152218
32.361160	1311.441142	17.157235
31.683307	1309.336547	17.162253
32.094729	1312.963254	17.167271
32.075538	1310.527160	17.172288
32.149079	1310.701238	17.177306
32.170225	1317.588161	17.182323
31.895169	1312.695675	17.187341
32.409595	1312.930999	17.192359
32.149479	1309.623403	17.197376
32.348074	1314.113284	17.202394
32.407791	1308.139801	17.207411
32.023890	1314.532387	17.212429
32.322590	1329.901107	17.217447
32.665208	1346.301523	17.222464
32.451062	1341.552482	17.227482
32.884678	1338.965425	17.232499
32.923600	1337.088195	17.237517
32.631206	1318.619757	17.242535
32.615920	1315.367681	17.247552
32.562093	1308.357513	17.252570
32.459013	1305.849879	17.257587
32.465834	1314.680464	17.262605
32.699893	1328.546536	17.267623
32.844575	1334.401224	17.272640
32.682708	1330.125802	17.277658
33.240224	1327.229655	17.282675
32.854249	1340.905105	17.287693
32.999418	1323.073642	17.292711
33.463094	1334.227353	17.297728
32.869061	1322.731141	17.302746
33.163684	1325.475244	17.307763
32.657629	1321.561139	17.312781
32.685297	1330.998109	17.317799
33.046310	1332.914310	17.322816
32.982028	1328.994769	17.327834
33.276056	1321.166384	17.332851
33.205369	1330.775541	17.337869
33.555434	1321.232405	17.342887
33.041587	1327.529981	17.347904
32.843118	1328.988440	17.352922
33.194128	1325.662325	17.357939
33.048244	1325.855807	17.362957
33.297645	1330.501843	17.367975
33.373652	1330.126707	17.372992
32.845961	1335.089601	17.378010
33.656779	1342.363878	17.383027
33.518990	1361.845760	17.388045
33.984160	1355.759061	17.393063
33.795596	1362.287822	17.398080
33.465305	1364.902735	17.403098
33.621367	1356.065702	17.408115
33.690942	1368.623248	17.413133
33.625359	1359.024506	17.418151
34.130482	1354.557141	17.423168
33.981150	1355.830699	17.428186
33.895276	1357.850427	17.433203
33.850088	1353.367494	17.438221
34.137655	1350.231008	17.443239
34.120327	1352.302375	17.448256
34.004273	1349.370908	17.453274
34.129704	1334.353269	17.458291
33.972337	1342.063444	17.463309
33.735983	1347.054478	17.468327
33.948873	1349.329846	17.473344
34.105638	1349.947221	17.478362
34.300758	1349.186622	17.483379
33.722245	1352.099320	17.488397
34.025131	1351.570084	17.493415
34.137385	1342.810783	17.498432
34.236868	1351.490615	17.503450
34.149639	1353.651115	17.508467
34.266769	1353.761678	17.513485
34.194055	1341.261828	17.518503
34.297152	1346.058863	17.523520
34.214387	1359.305785	17.528538
34.520336	1371.029329	17.533555
34.472876	1371.581310	17.538573
34.731780	1369.164119	17.543591
34.949252	1369.599399	17.548608
34.515034	1377.634561	17.553626
34.873572	1374.702456	17.558643
34.701842	1366.560626	17.563661
34.902153	1364.311402	17.568679
34.928240	1356.063201	17.573696
34.811270	1351.968918	17.578714
34.808698	1341.882597	17.583731
34.599671	1337.660650	17.588749
34.433470	1358.755858	17.593767
35.069701	1358.999361	17.598784
35.003844	1360.333899	17.603802
35.083402	1362.229780	17.608819
34.994508	1368.825110	17.613837
35.198078	1367.374542	17.618855
35.172573	1369.724032	17.623872
34.964568	1367.140063	17.628890
35.384077	1356.932664	17.633907
35.173261	1361.475389	17.638925
35.034796	1357.437418	17.643943
35.139099	1363.596041	17.648960
35.575271	1365.433661	17.653978
35.693089	1355.578573	17.658995
35.388583	1361.830082	17.664013
35.295387	1363.468747	17.669031
35.462243	1364.416728	17.674048
35.166949	1371.691104	17.679066
35.469374	1359.750764	17.684083
35.419924	1362.043589	17.689101
35.323640	1361.986738	17.694119
35.469397	1360.797313	17.699136
35.587324	1362.888805	17.704154
35.534028	1355.071457	17.709171
35.341761	1372.947054	17.714189
35.321810	1383.136414	17.719207
35.668785	1386.887981	17.724224
35.299021	1395.436879	17.729242
35.859418	1383.089245	17.734259
35.808063	1396.236905	17.739277
35.562655	1392.312694	17.744295
35.565739	1395.012565	17.749312
35.858505	1415.876345	17.754330
36.037483	1414.713305	17.759347
36.144454	1417.786916	17.764365
36.174977	1417.161833	17.769383
36.406090	1406.811977	17.774400
36.264051	1412.968890	17.779418
36.450837	1411.451807	17.784435
36.911372	1405.387510	17.789453
36.596480	1391.672624	17.794471
36.606428	1377.279172	17.799488
36.730114	1391.682464	17.804506
36.537231	1377.340313	17.809523
36.340868	1372.094233	17.814541
36.302060	1380.257228	17.819559
36.620303	1372.401973	17.824576
36.410294	1371.895064	17.829594
36.726896	1367.802606	17.834611
36.680812	1370.731869	17.839629
36.587270	1375.444153	17.844647
36.675158	1369.501413	17.849664
36.503126	1375.521549	17.854682
36.675664	1362.442500	17.859699
36.729393	1374.149937	17.864717
36.823734	1389.985617	17.869735
36.863333	1394.416023	17.874752
37.079953	1406.026435	17.879770
37.125098	1402.689926	17.884787
36.955997	1397.894433	17.889805
37.036728	1403.750681	17.894823
37.169919	1396.422109	17.899840
37.082968	1408.679628	17.904858
37.208929	1403.061274	17.909875
37.154624	1401.554192	17.914893
37.011995	1393.940589	17.919911
37.352776	1399.432916	17.924928
37.111016	1404.639821	17.929946
37.031363	1396.594931	17.934963
36.956392	1397.712087	17.939981
37.000014	1402.420958	17.944999
37.317049	1408.829802	17.950016
37.103125	1407.561350	17.955034
37.203249	1402.522068	17.960051
37.235141	1404.285298	17.965069
37.258219	1426.414985	17.970087
37.551218	1424.938187	17.975104
37.308507	1436.684520	17.980122
37.662503	1440.004236	17.985139
37.538431	1438.380751	17.990157
37.784049	1437.293681	17.995175
37.953151	1424.323809	18.000192
38.138049	1426.307372	18.005210
37.965868	1435.100737	18.010227
37.752954	1425.925947	18.015245
37.450822	1436.223088	18.020263
38.018572	1427.089898	18.025280
37.780078	1436.908400	18.030298
37.842115	1427.104235	18.035315
38.037489	1433.614335	18.040333
37.865668	1436.762852	18.045351
38.417833	1438.176164	18.050368
38.136799	1437.861719	18.055386
37.921889	1430.434867	18.060403
37.847950	1442.100504	18.065421
37.970859	1454.494960	18.070439
38.243148	1449.654711	18.075456
37.948978	1456.175802	18.080474
38.222709	1456.800192	18.085491
38.245041	1454.880027	18.090509
38.058591	1457.880580	18.095527
38.462990	1469.941042	18.100544
38.669686	1475.235916	18.105562
38.752473	1481.167049	18.110579
39.207182	1475.970607	18.115597
38.709827	1470.640869	18.120615
38.755508	1446.730942	18.125632
38.759119	1456.281813	18.130650
39.378627	1452.564761	18.135667
39.281504	1439.750374	18.140685
38.832703	1443.410102	18.145703
39.188219	1430.087710	18.150720
39.017768	1442.951591	18.155738
39.013514	1442.744858	18.160755
39.051765	1431.687562	18.165773
39.147680	1451.196606	18.170791
39.020684	1435.831301	18.175808
38.991784	1431.849577	18.180826
39.048933	1432.319280	18.185843
39.021845	1436.428462	18.190861
39.180052	1450.168624	18.195879
39.218556	1458.170434	18.200896
39.175794	1462.759771	18.205914
39.431596	1458.039964	18.210931
39.287287	1464.763406	18.215949
39.151028	1472.677234	18.220967
39.676138	1460.264911	18.225984
39.554307	1461.299282	18.231002
39.583198	1454.859200	18.236019
39.523342	1461.442675	18.241037
39.441939	1465.609676	18.246055
39.585816	1464.087489	18.251072
39.425142	1470.424673	18.256090
39.582112	1466.276338	18.261107
40.079383	1459.388233	18.266125
39.530292	1459.767769	18.271143
39.915736	1460.709877	18.276160
39.673556	1467.503857	18.281178
39.878732	1468.090780	18.286195
40.009570	1466.243591	18.291213
39.896477	1480.494049	18.296231
40.038952	1483.645652	18.301248
39.881974	1493.945568	18.306266
39.902166	1491.124976	18.311283
40.172965	1493.008105	18.316301
39.932552	1487.243696	18.321319
40.400329	1483.926952	18.326336
40.140890	1482.126273	18.331354
40.509087	1490.394372	18.336371
40.381103	1489.594747	18.341389
40.483487	1490.059718	18.346407
40.271134	1482.896587	18.351424
40.452322	1485.405962	18.356442
40.616882	1485.697253	18.361459
40.821828	1478.983525	18.366477
40.580610	1491.012718	18.371495
40.733697	1487.011476	18.376512
40.557470	1484.718678	18.381530
40.129672	1485.555684	18.386547
40.803602	1491.188548	18.391565
41.044395	1512.081930	18.396583
40.866030	1511.116633	18.401600
40.778800	1502.436729	18.406618
40.735507	1504.323049	18.411635
41.081593	1511.670028	18.416653
41.171007	1517.125280	18.421671
41.435896	1503.104060	18.426688
41.229620	1514.144820	18.431706
41.275795	1507.337291	18.436723
41.366089	1505.721218	18.441741
41.390553	1501.846386	18.446759
41.162046	1492.063910	18.451776
41.340299	1496.789493	18.456794
41.265377	1502.930604	18.461811
41.441301	1499.072820	18.466829
41.310362	1496.691814	18.471847
41.469214	1504.357977	18.476864
41.112270	1501.432509	18.481882
41.219480	1503.828941	18.486899
41.578155	1508.359301	18.491917
41.332683	1512.487734	18.496935
41.746246	1502.706417	18.501952
41.490473	1499.809472	18.506970
41.309304	1507.553591	18.511987
41.828082	1521.320332	18.517005
41.806516	1536.186782	18.522023
41.980013	1528.038884	18.527040
41.913879	1534.570281	18.532058
41.882712	1531.789288	18.537075
42.323686	1521.279805	18.542093
41.754877	1532.717217	18.547111
42.016717	1529.055040	18.552128
41.934404	1528.542336	18.557146
41.917041	1526.204724	18.562163
42.230584	1532.499239	18.567181
41.843820	1530.127123	18.572199
42.114188	1536.813430	18.577216
42.353683	1522.063728	18.582234
42.245312	1533.939069	18.587251
42.619245	1527.467022	18.592269
42.462056	1522.464007	18.597287
42.697072	1518.964146	18.602304
42.427161	1517.723852	18.607322
42.452737	1530.652197	18.612339
42.289736	1528.717829	18.617357
42.654063	1550.188833	18.622375
42.822531	1549.342087	18.627392
42.905201	1547.485935	18.632410
42.864180	1554.854119	18.637427
43.082683	1554.380188	18.642445
43.112782	1549.298910	18.647463
42.930118	1537.630878	18.652480
43.292685	1524.157240	18.657498
43.080743	1522.742388	18.662515
43.177732	1510.663903	18.667533
43.352436	1514.396390	18.672551
43.137864	1519.514579	18.677568
43.017069	1511.644943	18.682586
42.647108	1520.148273	18.687603
43.007572	1521.335858	18.692621
43.101077	1539.719441	18.697639
43.119422	1542.246733	18.702656
43.316935	1549.032904	18.707674
43.073637	1551.138564	18.712691
43.285586	1540.194160	18.717709
43.179499	1553.708887	18.722727
43.328775	1551.978712	18.727744
43.500880	1560.923801	18.732762
43.273599	1570.635807	18.737779
43.589762	1573.285051	18.742797
43.455653	1576.661208	18.747815
43.577812	1578.086680	18.752832
44.076392	1578.796678	18.757850
43.724320	1578.999107	18.762867
43.870050	1577.542743	18.767885
44.148859	1578.456060	18.772903
43.906632	1572.561998	18.777920
43.928008	1562.848337	18.782938
44.027476	1562.633483	18.787955
44.122971	1563.977148	18.792973
44.271163	1568.354584	18.797991
44.101557	1571.324416	18.803008
44.121264	1570.194823	18.808026
44.348352	1572.972201	18.813043
44.491345	1581.402441	18.818061
44.209547	1590.517978	18.823079
44.745868	1592.061881	18.828096
44.884526	1580.602422	18.833114
44.305582	1570.088557	18.838131
44.670882	1561.722270	18.843149
44.772094	1570.343278	18.848167
44.531667	1568.731959	18.853184
45.040667	1565.772150	18.858202
44.606845	1569.980997	18.863219
44.590460	1564.884970	18.868237
45.051818	1585.977756	18.873255
45.073858	1588.007991	18.878272
45.260970	1576.128704	18.883290
44.939875	1571.150845	18.888307
45.054274	1568.397318	18.893325
44.958425	1565.441203	18.898343
44.723032	1577.878945	18.903360
45.158944	1584.292195	18.908378
44.870336	1588.425428	18.913395
45.631204	1586.679809	18.918413
45.219038	1591.544521	18.923431
45.155681	1593.546771	18.928448
45.498463	1590.932982	18.933466
45.540320	1588.437524	18.938483
45.236961	1587.824411	18.943501
45.352311	1590.642735	18.948519
45.421120	1586.199913	18.953536
45.527314	1582.491842	18.958554
45.569358	1587.044732	18.963571
45.246153	1586.855376	18.968589
45.156843	1585.468244	18.973607
45.185222	1591.919055	18.978624
45.642220	1603.362649	18.983642
45.554603	1608.334257	18.988659
46.084219	1610.480056	18.993677
46.031841	1609.554127	18.998695
45.966539	1618.648401	19.003712
46.358506	1607.496190	19.008730
45.862485	1612.864948	19.013747
46.195627	1606.687810	19.018765
46.074983	1608.468052	19.023783
46.129660	1605.993697	19.028800
46.168068	1602.349207	19.033818
46.073441	1600.727916	19.038835
46.496448	1600.880748	19.043853
46.222866	1598.181614	19.048871
46.154208	1594.826900	19.053888
46.757679	1592.498291	19.058906
46.071396	1604.991027	19.063923
46.311333	1611.574926	19.068941
46.647941	1619.274312	19.073959
46.410257	1631.673893	19.078976
46.612867	1619.585315	19.083994
46.747791	1633.549179	19.089011
46.545269	1630.286701	19.094029
46.672123	1629.063378	19.099047
46.444445	1636.184162	19.104064
47.012494	1625.048847	19.109082
46.495329	1634.717159	19.114099
46.751172	1648.759440	19.119117
46.922266	1657.964987	19.124135
46.968298	1665.402668	19.129152
47.276543	1662.525688	19.134170
47.229115	1661.750511	19.139187
47.315781	1651.929527	19.144205
47.380408	1652.868470	19.149223
47.342303	1654.861429	19.154240
47.388423	1655.789656	19.159258
46.985651	1660.758739	19.164275
47.270346	1655.631728	19.169293
47.618173	1652.392685	19.174311
47.226608	1660.781952	19.179328
47.728059	1665.764702	19.184346
47.890412	1686.305166	19.189363
47.683766	1679.087062	19.194381
48.198320	1679.839303	19.199399
48.108027	1676.112563	19.204416
48.127905	1650.498722	19.209434
48.018816	1651.981781	19.214451
47.814770	1652.619542	19.219469
48.077964	1644.369723	19.224487
47.574149	1657.394492	19.229504
48.020585	1670.187914	19.234522
48.219368	1684.303061	19.239539
48.229128	1681.032194	19.244557
48.281993	1681.303795	19.249575
48.395750	1683.032636	19.254592
48.756592	1665.177274	19.259610
48.370423	1681.325098	19.264627
48.286921	1671.453537	19.269645
48.852264	1675.902484	19.274663
48.100414	1676.159297	19.279680
48.250734	1671.580120	19.284698
48.485849	1672.085323	19.289715
48.702331	1668.629443	19.294733
48.802911	1667.372279	19.299751
48.467384	1677.555817	19.304768
48.723513	1667.261882	19.309786
48.916035	1672.056023	19.314803
48.596467	1673.359368	19.319821
49.089224	1672.077031	19.324839
48.693411	1665.859152	19.329856
48.821533	1673.556078	19.334874
48.778019	1692.031821	19.339891
49.114046	1690.419922	19.344909
49.362207	1684.229659	19.349927
49.011320	1687.720868	19.354944
49.531492	1684.747377	19.359962
49.250046	1684.393230	19.364979
49.182803	1687.180387	19.369997
49.600149	1693.053844	19.375015
49.521825	1692.229844	19.380032
49.641487	1694.576212	19.385050
49.731550	1698.735358	19.390067
49.646566	1693.339229	19.395085
49.821608	1689.874458	19.400103
49.772412	1678.388157	19.405120
49.660569	1677.666559	19.410138
49.691744	1668.406327	19.415155
49.687920	1679.980218	19.420173
49.690169	1680.120829	19.425191
49.611539	1693.785856	19.430208
49.856274	1701.077267	19.435226
49.872271	1705.569544	19.440243
49.633755	1708.702781	19.445261
50.270663	1702.908379	19.450279
49.794466	1708.824675	19.455296
50.022700	1707.965663	19.460314
50.432208	1716.472320	19.465331
50.583635	1729.662671	19.470349
50.579030	1736.682785	19.475367
50.619750	1740.056408	19.480384
50.645000	1723.197100	19.485402
50.782117	1733.206746	19.490419
50.509560	1735.318062	19.495437
50.774099	1728.543179	19.500455
51.005909	1727.686723	19.505472
50.972671	1725.811553	19.510490
50.900878	1729.434906	19.515507
50.828927	1724.054325	19.520525
50.919864	1729.440896	19.525543
50.643933	1734.752780	19.530560
50.778543	1720.507266	19.535578
50.737511	1727.890101	19.540595
50.888601	1725.972993	19.545613
51.292547	1715.815575	19.550631
50.910645	1719.751297	19.555648
51.307187	1720.493554	19.560666
51.499637	1727.951509	19.565683
51.252421	1727.687757	19.570701
51.136168	1740.659446	19.575719
51.303750	1744.037655	19.580736
51.728137	1750.087921	19.585754
51.758212	1748.871165	19.590771
51.153703	1755.060693	19.595789
51.700368	1751.166264	19.600807
51.546651	1748.220484	19.605824
51.804933	1749.652960	19.610842
51.845118	1732.480145	19.615859
51.663051	1746.350928	19.620877
51.782438	1743.697331	19.625895
51.949821	1746.420847	19.630912
51.691988	1743.115928	19.635930
51.914179	1750.778026	19.640947
52.185445	1764.735969	19.645965
52.568112	1760.047034	19.650983
52.248057	1763.352445	19.656000
52.612458	1752.230287	19.661018
52.940544	1754.691761	19.666035
52.474701	1745.226376	19.671053
52.293170	1732.462336	19.676071
52.235912	1734.147058	19.681088
52.275406	1740.016167	19.686106
52.450984	1760.607690	19.691123
52.377469	1762.377785	19.696141
52.484261	1751.712456	19.701159
52.432206	1761.769585	19.706176
52.417390	1760.671285	19.711194
52.445096	1762.723833	19.716211
52.761791	1781.806185	19.721229
53.207105	1782.933285	19.726247
53.145221	1785.886896	19.731264
52.905385	1791.332588	19.736282
52.919694	1785.951483	19.741299
53.124516	1790.288109	19.746317
53.163398	1783.696629	19.751335
53.286814	1777.489582	19.756352
53.303624	1785.214444	19.761370
53.449987	1771.653949	19.766387
53.255533	1783.250820	19.771405
53.435238	1781.015185	19.776423
53.277708	1778.105464	19.781440
53.439533	1794.673302	19.786458
53.670917	1799.886642	19.791475
53.448253	1811.190958	19.796493
54.179849	1805.082020	19.801511
53.764381	1814.281238	19.806528
53.918006	1807.889648	19.811546
54.100851	1800.258568	19.816563
53.888122	1804.796620	19.821581
54.062486	1800.135471	19.826599
54.108600	1794.700277	19.831616
53.968779	1795.242763	19.836634
53.943576	1790.754031	19.841651
53.811426	1798.164192	19.846669
54.170242	1801.565474	19.851687
53.971827	1821.075293	19.856704
54.213873	1838.824788	19.861722
54.491464	1847.029735	19.866739
54.732810	1837.471214	19.871757
54.814586	1836.657706	19.876775
55.021530	1842.563302	19.881792
54.997451	1839.242099	19.886810
55.627024	1846.185997	19.891827
55.166684	1826.457738	19.896845
55.568224	1801.472585	19.901863
55.312817	1802.133816	19.906880
55.228414	1802.547439	19.911898
55.533799	1802.114628	19.916915
55.360811	1806.684683	19.921933
55.125083	1797.293762	19.926951
55.471652	1801.405346	19.931968
54.710049	1808.424454	19.936986
55.101916	1801.917829	19.942003
55.081600	1800.225550	19.947021
55.440677	1792.716870	19.952039
55.367104	1792.978699	19.957056
55.331280	1791.513007	19.962074
55.293717	1806.069764	19.967091
55.336140	1789.651245	19.972109
55.223452	1790.203804	19.977127
55.290914	1815.224356	19.982144
55.404877	1817.285070	19.987162
55.485092	1828.401453	19.992179
55.571560	1833.550215	19.997197
55.683013	1840.370448	20.002215
55.382276	1836.394653	20.007232
55.750670	1856.211457	20.012250
56.183017	1853.088303	20.017267
55.695211	1860.308559	20.022285
56.090949	1851.129195	20.027303
56.314304	1853.211960	20.032320
56.363818	1847.408858	20.037338
56.659536	1849.830826	20.042355
56.198095	1850.574992	20.047373
56.314539	1846.010035	20.052391
56.622282	1847.107950	20.057408
56.167114	1849.504638	20.062426
56.619104	1864.439058	20.067443
56.531658	1875.837174	20.072461
56.981239	1875.295445	20.077479
56.648433	1883.881010	20.082496
56.944538	1875.517352	20.087514
56.926690	1877.736515	20.092531
57.070970	1878.494564	20.097549
57.304001	1872.931937	20.102567
57.435161	1870.616925	20.107584
57.163851	1874.328859	20.112602
57.487725	1865.971632	20.117619
57.287179	1876.590829	20.122637
57.246062	1868.480257	20.127655
57.397521	1871.430450	20.132672
57.286302	1871.987887	20.137690
57.038962	1860.421660	20.142707
57.001531	1873.185525	20.147725
57.288984	1883.350693	20.152743
57.244753	1893.027078	20.157760
57.428683	1896.191588	20.162778
57.750323	1892.813918	20.167795
57.379769	1899.617135	20.172813
57.726221	1895.942438	20.177831
57.932382	1904.315938	20.182848
58.052385	1924.325927	20.187866
58.305443	1913.604773	20.192883
58.165935	1927.695052	20.197901
58.290037	1921.728389	20.202919
58.737860	1925.132679	20.207936
58.436436	1915.175391	20.212954
58.675436	1898.340345	20.217971
58.519165	1881.084538	20.222989
58.617919	1881.965087	20.228007
58.588650	1879.174269	20.233024
58.260203	1886.889811	20.238042
58.647240	1902.697632	20.243059
58.662425	1919.898161	20.248077
59.215125	1919.010612	20.253095
59.168786	1915.941900	20.258112
58.894578	1931.053713	20.263130
58.819158	1908.927719	20.268147
58.845691	1908.298160	20.273165
58.966559	1919.984263	20.278183
58.851112	1915.469098	20.283200
58.886881	1921.565668	20.288218
59.378995	1917.477079	20.293235
58.928350	1922.256529	20.298253
59.136751	1912.254198	20.303271
59.443639	1908.280140	20.308288
59.242770	1913.965882	20.313306
59.369569	1916.347717	20.318323
59.179523	1926.354965	20.323341
59.292906	1928.342954	20.328359
59.569374	1941.450970	20.333376
59.671110	1936.539597	20.338394
59.873513	1932.439130	20.343411
59.720744	1938.247234	20.348429
59.813911	1936.437330	20.353447
59.861520	1920.131989	20.358464
59.643857	1939.785698	20.363482
59.697983	1952.178162	20.368499
59.831245	1957.201106	20.373517
60.205405	1963.515683	20.378535
60.270811	1968.063242	20.383552
60.211039	1963.988066	20.388570
60.443304	1963.737046	20.393587
60.057320	1961.713950	20.398605
60.296257	1964.104391	20.403623
60.936015	1966.804064	20.408640
60.752973	1974.486125	20.413658
60.805857	1971.866731	20.418675
60.716335	1972.062698	20.423693
60.777273	1980.192563	20.428711
61.267795	1978.205049	20.433728
61.191050	1981.038715	20.438746
61.240161	1971.701709	20.443763
61.236057	1961.704216	20.448781
61.523748	1952.073778	20.453799
61.324564	1946.275990	20.458816
60.895788	1947.239952	20.463834
60.967743	1959.717268	20.468851
60.909950	1972.408994	20.473869
60.943612	1978.829170	20.478887
61.098197	1978.324077	20.483904
60.994552	1990.354105	20.488922
61.222316	2002.981645	20.493939
61.236941	2011.150298	20.498957
61.815545	2005.137089	20.503975
61.848081	1995.093351	20.508992
61.990782	2007.495604	20.514010
62.149835	2004.684999	20.519027
62.001276	2006.980549	20.524045
61.941473	2007.094823	20.529063
62.349836	1996.342386	20.534080
62.459889	2001.785336	20.539098
62.324618	1992.872949	20.544115
62.158335	1999.388051	20.549133
62.141329	2001.287008	20.554151
62.304319	1999.844677	20.559168
62.214558	2023.673068	20.564186
62.418976	2018.117883	20.569203
62.760078	2021.289859	20.574221
62.948709	2025.629627	20.579239
63.218114	2027.131550	20.584256
62.721513	2032.346604	20.589274
62.997304	2024.172849	20.594291
62.919300	2028.592199	20.599309
62.767081	2023.361422	20.604327
63.057735	2017.215174	20.609344
63.092356	2020.270964	20.614362
63.084940	2021.029728	20.619379
62.774637	2016.225136	20.624397
62.896741	2018.710523	20.629415
62.911947	2023.447517	20.634432
63.002661	2038.746655	20.639450
63.597439	2047.448022	20.644467
63.367246	2041.130124	20.649485
63.057108	2044.044178	20.654503
63.383091	2048.128921	20.659520
63.339960	2051.673586	20.664538
63.491671	2058.077398	20.669555
63.436151	2069.236900	20.674573
63.738506	2072.142462	20.679591
64.153926	2068.874427	20.684608
64.300817	2075.568421	20.689626
64.411096	2072.700524	20.694643
64.233507	2068.289307	20.699661
64.206503	2076.409373	20.704679
64.656716	2070.159518	20.709696
64.380140	2079.283531	20.714714
64.393345	2067.606290	20.719731
64.922233	2073.815371	20.724749
64.463072	2069.795272	20.729767
64.943375	2061.948667	20.734784
64.603539	2069.687051	20.739802
65.089443	2061.005641	20.744819
64.716139	2066.533370	20.749837
65.047944	2063.394932	20.754855
65.131676	2061.538937	20.759872
64.725115	2075.692858	20.764890
64.818604	2069.573330	20.769907
65.178312	2063.371141	20.774925
65.162847	2066.440351	20.779943
65.069397	2052.819316	20.784960
65.362272	2063.079377	20.789978
65.279136	2056.782400	20.794995
65.176914	2072.391870	20.800013
65.448771	2091.544234	20.805031
65.297086	2090.920553	20.810048
65.584716	2095.100638	20.815066
66.029852	2090.491029	20.820083
65.520685	2094.967614	20.825101
65.702951	2093.970914	20.830119
66.000375	2088.414084	20.835136
65.817661	2094.634695	20.840154
65.706377	2086.992725	20.845171
66.094422	2098.111089	20.850189
66.119325	2105.053647	20.855207
66.494912	2099.981129	20.860224
66.036246	2102.537493	20.865242
65.916527	2108.631534	20.870259
66.298536	2107.855704	20.875277
66.115200	2105.135238	20.880295
66.171202	2109.270605	20.885312
66.431389	2122.516120	20.890330
66.547338	2128.911709	20.895347
66.665457	2130.427668	20.900365
66.539077	2140.555223	20.905383
66.815021	2135.665732	20.910400
66.596300	2139.695409	20.915418
66.861156	2142.360729	20.920435
66.905589	2149.359523	20.925453
66.977519	2165.387115	20.930471
67.341957	2155.850934	20.935488
67.180455	2165.315796	20.940506
67.178991	2159.287153	20.945523
67.430218	2153.273762	20.950541
67.591823	2157.126295	20.955559
67.627354	2161.673346	20.960576
67.453008	2153.618937	20.965594
67.704959	2153.522140	20.970611
67.888629	2144.664734	20.975629
67.620484	2154.714587	20.980647
67.955515	2154.668997	20.985664
67.899311	2158.253647	20.990682
67.750935	2155.482894	20.995699
68.061832	2163.628556	21.000717
68.388055	2178.204958	21.005735
68.535174	2180.094872	21.010752
68.345919	2171.992921	21.015770
68.436573	2174.953634	21.020787
68.663255	2175.208669	21.025805
68.741972	2172.027860	21.030823
68.796340	2154.091577	21.035840
68.573261	2148.461454	21.040858
68.580006	2153.904240	21.045875
68.596668	2154.203891	21.050893
68.526535	2171.243229	21.055911
69.191299	2173.084837	21.060928
68.834800	2178.320838	21.065946
68.924579	2172.087313	21.070963
69.618147	2164.720323	21.075981
69.595211	2175.602451	21.080999
69.228358	2169.744936	21.086016
69.464508	2167.452262	21.091034
69.461964	2159.553268	21.096051
69.482011	2171.302712	21.101069
69.325965	2164.528772	21.106087
69.346766	2161.746542	21.111104
69.356987	2166.704884	21.116122
69.369480	2164.077577	21.121139
69.685139	2166.926622	21.126157
69.453510	2190.187401	21.131175
69.800533	2190.787090	21.136192
69.944818	2186.452471	21.141210
69.637339	2188.508210	21.146227
69.999248	2184.405283	21.151245
70.250049	2189.246237	21.156263
70.036753	2195.888501	21.161280
70.167048	2222.316280	21.166298
70.165532	2217.003396	21.171315
70.362902	2213.214723	21.176333
70.024160	2217.047356	21.181351
70.461043	2205.194741	21.186368
70.587921	2217.671044	21.191386
70.251017	2235.934191	21.196403
71.182169	2244.475642	21.201421
71.164405	2245.608190	21.206439
71.060820	2241.916193	21.211456
71.281987	2234.593134	21.216474
71.591064	2235.943623	21.221491
71.581604	2228.000855	21.226509
71.240564	2225.428530	21.231527
71.830260	2234.862761	21.236544
71.998388	2221.823093	21.241562
71.881209	2206.208933	21.246579
71.882941	2194.700431	21.251597
71.411497	2197.147898	21.256615
71.542390	2193.340314	21.261632
71.743372	2201.297102	21.266650
71.857811	2217.000769	21.271667
71.916742	2215.745340	21.276685
72.048548	2236.698299	21.281703
72.126908	2228.959109	21.286720
72.064343	2228.471458	21.291738
71.998784	2223.275479	21.296755
71.996098	2219.735290	21.301773
71.659672	2223.878575	21.306791
72.275308	2214.733458	21.311808
72.202081	2229.444160	21.316826
72.315649	2250.931279	21.321843
72.376041	2244.593532	21.326861
72.406280	2268.000839	21.331879
72.597413	2253.261996	21.336896
72.491133	2253.972572	21.341914
72.495305	2258.532323	21.346931
72.276352	2264.494425	21.351949
72.529791	2275.227315	21.356967
72.769774	2287.538092	21.361984
72.824097	2282.742732	21.367002
73.223941	2287.487384	21.372019
73.579766	2297.079278	21.377037
73.402515	2313.500655	21.382055
73.411758	2306.550854	21.387072
73.663962	2310.231332	21.392090
73.722260	2307.383810	21.397107
73.814894	2311.493874	21.402125
73.958737	2303.690259	21.407143
74.100553	2303.421532	21.412160
74.011329	2306.343940	21.417178
74.006593	2300.808324	21.422195
74.455979	2303.501783	21.427213
74.041664	2300.038392	21.432231
74.415204	2297.139071	21.437248
74.628539	2297.225052	21.442266
74.238509	2302.556807	21.447283
74.636310	2289.997184	21.452301
74.214094	2296.910311	21.457319
74.237879	2301.086105	21.462336
74.296640	2300.088974	21.467354
73.973615	2303.687520	21.472371
74.443953	2313.530553	21.477389
74.350322	2325.360749	21.482407
74.636434	2314.968901	21.487424
74.507441	2328.091620	21.492442
74.672158	2350.830696	21.497459
75.124537	2342.297208	21.502477
75.144649	2360.963613	21.507495
75.173552	2360.889966	21.512512
75.143722	2354.799012	21.517530
75.433391	2354.960549	21.522547
75.862096	2358.707094	21.527565
75.572505	2364.886843	21.532583
75.822349	2365.770753	21.537600
75.901652	2368.081779	21.542618
75.940176	2378.619213	21.547635
76.199006	2365.887649	21.552653
76.093661	2370.278550	21.557671
76.287411	2371.666651	21.562688
76.424713	2368.037894	21.567706
76.006848	2378.236701	21.572723
76.154180	2361.641933	21.577741
76.219461	2367.664104	21.582759
76.146625	2364.564650	21.587776
76.664539	2362.908396	21.592794
76.105488	2367.676006	21.597811
76.709472	2376.847317	21.602829
76.745544	2392.057027	21.607847
76.906363	2392.967490	21.612864
77.124516	2383.527442	21.617882
77.195128	2391.993731	21.622899
77.140548	2385.462749	21.627917
77.123851	2385.297435	21.632935
77.177612	2381.993149	21.637952
77.602810	2385.640278	21.642970
77.330224	2382.947925	21.647987
77.522123	2388.738107	21.653005
77.526993	2396.703449	21.658023
77.703602	2389.951895	21.663040
78.020540	2379.728529	21.668058
77.599532	2390.537734	21.673075
77.854814	2379.680454	21.678093
77.892851	2384.898051	21.683111
77.514197	2378.083312	21.688128
77.609900	2384.560709	21.693146
77.983127	2407.970890	21.698163
77.917590	2406.563604	21.703181
78.064910	2418.683519	21.708199
78.152250	2410.095074	21.713216
78.492482	2405.707084	21.718234
78.202127	2414.312289	21.723251
78.392572	2406.046555	21.728269
78.734283	2426.518539	21.733287
78.650646	2441.057533	21.738304
78.769190	2439.390621	21.743322
78.986560	2446.443204	21.748339
78.761140	2438.917207	21.753357
78.895233	2440.472286	21.758375
79.170858	2443.111859	21.763392
79.053756	2440.762669	21.768410
79.156976	2439.040023	21.773427
79.261402	2446.649128	21.778445
79.299199	2450.000554	21.783463
79.654258	2448.338184	21.788480
79.906929	2456.106615	21.793498
79.631828	2451.798051	21.798515
79.944808	2445.982208	21.803533
80.092661	2450.285145	21.808551
79.388416	2455.992613	21.813568
79.835003	2448.602603	21.818586
79.829862	2454.839233	21.823603
80.060334	2455.432640	21.828621
80.171526	2470.008699	21.833639
79.963187	2480.917800	21.838656
80.659608	2480.454877	21.843674
80.606767	2471.287215	21.848691
80.619248	2463.576140	21.853709
80.821394	2471.699812	21.858727
80.648445	2478.085896	21.863744
80.955385	2463.889126	21.868762
80.579918	2468.814568	21.873779
80.714276	2468.695506	21.878797
81.173009	2476.064851	21.883815
81.342511	2489.333963	21.888832
81.127642	2486.220991	21.893850
81.189215	2496.909421	21.898867
80.919600	2486.198819	21.903885
81.315553	2494.955410	21.908903
81.146304	2497.965911	21.913920
81.495494	2494.999322	21.918938
81.405085	2518.520294	21.923955
81.425203	2525.384300	21.928973
82.076003	2521.678361	21.933991
81.844508	2528.452525	21.939008
82.109391	2520.273624	21.944026
82.078089	2514.179702	21.949043
82.324871	2512.064755	21.954061
82.298274	2520.203097	21.959079
82.141591	2519.158548	21.964096
82.474580	2526.394004	21.969114
82.359280	2539.485892	21.974131
82.507939	2545.119109	21.979149
82.835889	2551.064395	21.984167
82.678112	2547.531699	21.989184
83.059542	2543.227012	21.994202
82.994662	2550.385039	21.999219
82.883183	2534.730626	22.004237
83.210637	2539.516084	22.009255
82.813812	2539.171567	22.014272
83.277798	2528.068987	22.019290
83.247715	2530.011120	22.024307
83.263005	2526.654116	22.029325
83.190488	2547.614551	22.034343
83.514510	2558.875746	22.039360
83.618095	2556.286050	22.044378
83.419076	2566.139278	22.049395
83.498149	2563.385519	22.054413
83.726216	2568.905592	22.059431
83.649537	2572.579559	22.064448
83.994272	2578.921705	22.069466
83.712640	2588.963045	22.074483
84.241915	2593.083571	22.079501
84.294476	2587.457259	22.084519
83.790877	2593.616229	22.089536
84.415045	2582.132738	22.094554
84.606119	2593.010041	22.099571
84.371795	2620.326868	22.104589
84.956596	2616.840902	22.109607
84.986532	2626.364904	22.114624
85.024229	2609.145074	22.119642
85.143968	2618.745940	22.124659
85.322988	2615.049585	22.129677
85.449299	2609.273644	22.134695
85.312274	2608.409310	22.139712
85.561987	2596.440531	22.144730
85.540265	2601.337761	22.149747
85.330700	2609.948201	22.154765
85.467280	2608.382228	22.159783
85.251239	2615.008587	22.164800
85.341226	2611.980162	22.169818
85.686847	2635.157841	22.174835
85.976853	2636.748940	22.179853
86.123669	2634.978108	22.184871
85.819004	2643.564940	22.189888
86.083864	2639.893345	22.194906
85.677705	2652.406281	22.199923
85.984008	2657.363005	22.204941
86.304947	2670.432777	22.209959
86.316393	2674.175647	22.214976
86.526811	2673.283313	22.219994
86.560886	2677.813038	22.225011
86.668247	2686.401758	22.230029
86.968260	2689.731476	22.235047
87.021922	2691.685355	22.240064
87.066473	2686.079626	22.245082
87.628303	2688.718710	22.250099
87.322026	2684.757390	22.255117
87.683619	2685.018448	22.260135
87.810966	2685.008427	22.265152
87.872644	2675.773255	22.270170
88.121162	2681.881359	22.275187
87.966086	2679.350218	22.280205
88.008779	2683.893086	22.285223
87.949234	2681.691819	22.290240
87.899579	2677.894325	22.295258
88.021432	2675.688223	22.300275
88.226511	2677.468597	22.305293
88.175694	2670.331714	22.310311
87.825095	2672.944294	22.315328
88.105195	2671.057684	22.320346
88.192971	2674.250480	22.325363
88.206780	2688.122348	22.330381
88.400297	2690.204263	22.335399
88.556975	2707.929517	22.340416
88.493993	2699.136653	22.345434
88.473290	2700.893384	22.350451
88.693791	2701.308519	22.355469
89.135769	2706.996781	22.360487
88.970091	2726.585389	22.365504
89.145585	2726.005548	22.370522
88.991061	2725.505546	22.375539
89.211194	2735.087106	22.380557
89.368869	2727.707790	22.385575
89.101497	2726.013399	22.390592
89.706553	2740.967029	22.395610
89.989180	2749.921674	22.400627
89.860720	2749.466571	22.405645
90.291225	2745.760439	22.410663
89.909094	2760.750755	22.415680
90.321782	2758.530743	22.420698
90.276312	2752.857212	22.425715
90.242919	2746.100901	22.430733
90.766534	2748.627023	22.435751
90.512998	2752.431108	22.440768
90.396365	2749.679009	22.445786
90.243937	2740.261123	22.450803
90.197497	2749.767135	22.455821
90.757770	2757.650943	22.460839
90.651236	2776.900665	22.465856
91.012641	2782.559773	22.470874
91.148906	2781.795466	22.475891
91.103079	2771.240936	22.480909
91.241084	2777.087040	22.485927
91.043406	2780.432246	22.490944
91.518250	2791.811169	22.495962
91.724369	2800.313123	22.500979
91.398618	2813.094390	22.505997
91.444554	2798.696419	22.511015
91.625144	2811.760807	22.516032
91.791861	2800.569842	22.521050
91.937747	2809.781037	22.526067
91.842992	2822.343738	22.531085
92.390883	2815.515960	22.536103
92.069912	2830.299351	22.541120
92.291952	2826.157602	22.546138
92.265881	2827.758138	22.551155
92.313397	2826.908516	22.556173
92.526703	2842.059792	22.561191
92.623233	2855.586986	22.566208
92.908570	2847.370667	22.571226
92.763276	2842.127048	22.576243
92.732977	2845.669375	22.581261
93.136496	2848.425650	22.586279
93.249731	2852.267860	22.591296
93.216432	2874.383745	22.596314
93.204316	2872.696685	22.601331
93.258494	2885.667883	22.606349
93.880111	2871.724966	22.611367
93.548777	2881.160896	22.616384
93.789125	2881.805052	22.621402
93.901594	2882.026646	22.626419
93.383030	2881.161289	22.631437
93.889391	2893.265439	22.636455
94.202009	2910.038260	22.641472
94.045505	2907.111224	22.646490
94.431358	2899.651525	22.651507
94.241636	2903.371059	22.656525
94.596215	2897.063873	22.661543
94.571709	2917.017172	22.666560
94.751666	2920.525098	22.671578
95.027881	2925.497126	22.676595
95.324461	2915.877224	22.681613
95.206319	2923.376944	22.686631
95.155584	2920.576499	22.691648
95.279870	2912.778181	22.696666
95.786285	2913.648387	22.701683
95.065128	2912.676008	22.706701
95.711147	2901.309937	22.711719
95.576174	2906.889451	22.716736
95.582023	2903.808754	22.721754
95.862881	2909.401711	22.726771
95.671420	2904.911048	22.731789
95.821923	2902.349750	22.736807
95.645600	2905.215031	22.741824
95.617537	2908.238851	22.746842
95.844998	2924.587958	22.751859
95.859337	2940.847949	22.756877
95.970513	2935.058251	22.761895
96.113791	2954.921609	22.766912
96.251801	2972.564420	22.771930
96.561286	2964.119615	22.776947
96.743551	2970.191948	22.781965
97.065702	2962.965225	22.786983
97.091803	2965.229633	22.792000
96.911708	2963.923554	22.797018
97.315799	2970.611969	22.802035
97.262963	2991.400437	22.807053
97.552194	2989.412269	22.812071
97.218697	3002.115438	22.817088
97.459116	2988.949766	22.822106
97.957325	2987.595559	22.827123
97.792993	2997.479538	22.832141
98.088920	2985.986316	22.837159
97.958347	2996.056453	22.842176
98.182105	2985.178774	22.847194
97.982017	2967.609695	22.852211
98.404164	2993.178980	22.857229
98.270740	3009.480831	22.862247
98.432697	3013.164608	22.867264
98.657500	3011.863540	22.872282
98.901799	3003.025929	22.877299
98.545291	3016.790096	22.882317
98.655314	3010.836767	22.887335
98.736333	3012.159333	22.892352
98.834874	3028.705500	22.897370
99.047795	3033.929796	22.902387
98.933949	3051.178531	22.907405
99.401944	3040.765538	22.912423
99.590819	3041.610761	22.917440
99.282714	3042.937120	22.922458
99.535042	3038.516655	22.927475
99.474340	3062.613106	22.932493
99.488659	3060.727931	22.937511
99.540667	3065.193771	22.942528
99.922030	3068.063607	22.947546
99.906363	3061.551490	22.952563
99.972595	3091.975170	22.957581
100.192014	3085.443809	22.962599
100.552336	3093.730612	22.967616
100.507881	3093.847470	22.972634
100.634778	3085.925001	22.977651
100.868357	3088.870888	22.982669
101.102070	3082.046189	22.987687
100.993180	3095.930467	22.992704
101.099069	3093.373375	22.997722
101.544935	3105.018767	23.002739
101.068007	3115.648340	23.007757
101.333466	3113.019152	23.012775
101.612100	3107.965909	23.017792
101.271257	3112.335767	23.022810
101.776160	3110.741443	23.027827
101.801658	3117.747746	23.032845
101.683809	3107.578963	23.037863
102.022895	3110.419582	23.042880
101.989579	3104.818721	23.047898
102.056823	3099.912300	23.052915
101.581521	3113.177275	23.057933
102.033604	3127.203763	23.062951
102.242315	3132.436270	23.067968
102.361384	3128.404806	23.072986
102.347872	3137.121278	23.078003
102.485402	3148.164936	23.083021
102.655113	3162.107879	23.088039
102.720501	3160.332752	23.093056
102.920808	3166.819931	23.098074
103.273530	3158.250923	23.103091
103.157747	3155.792339	23.108109
103.220668	3151.377215	23.113127
103.511111	3161.598247	23.118144
103.357832	3183.426137	23.123162
103.921471	3177.668141	23.128179
103.867813	3187.262631	23.133197
104.013464	3174.207384	23.138215
104.024331	3175.002945	23.143232
103.664057	3177.556178	23.148250
104.329065	3179.239988	23.153267
104.261425	3178.451150	23.158285
104.397065	3183.434330	23.163303
104.410087	3194.038355	23.168320
104.438226	3199.912652	23.173338
104.731946	3195.926278	23.178355
104.357119	3205.541272	23.183373
104.466687	3201.557431	23.188391
104.707615	3219.842996	23.193408
104.976935	3228.272510	23.198426
105.028573	3217.038090	23.203443
105.178164	3228.306208	23.208461
105.261002	3228.153936	23.213479
105.401283	3242.050244	23.218496
105.743127	3249.651932	23.223514
105.673459	3245.557977	23.228531
105.872248	3241.914900	23.233549
105.839660	3253.066334	23.238567
106.265875	3243.486192	23.243584
105.906487	3252.661608	23.248602
106.563641	3260.839114	23.253619
106.620100	3280.247135	23.258637
106.681186	3276.062618	23.263655
106.846735	3266.980784	23.268672
106.726338	3278.524765	23.273690
107.215693	3272.451835	23.278707
107.144720	3274.479184	23.283725
107.080939	3266.247607	23.288743
107.056919	3266.330765	23.293760
107.035462	3267.632914	23.298778
107.210781	3261.606075	23.303795
107.532159	3279.496856	23.308813
107.482392	3291.166568	23.313831
107.630561	3293.433257	23.318848
107.510807	3293.476748	23.323866
107.627600	3286.841415	23.328883
107.360485	3301.295040	23.333901
107.923241	3312.838550	23.338919
108.251846	3314.041009	23.343936
107.897609	3323.377047	23.348954
108.244438	3321.520656	23.353971
108.595032	3324.165296	23.358989
108.774616	3340.697588	23.364007
108.985748	3338.447476	23.369024
109.110366	3344.829925	23.374042
109.377722	3330.736574	23.379059
109.225361	3326.611401	23.384077
109.162849	3319.964004	23.389095
109.059532	3319.336987	23.394112
109.100517	3341.146716	23.399130
109.406653	3334.942268	23.404147
109.425956	3339.538418	23.409165
109.331890	3332.867103	23.414183
109.902304	3342.383169	23.419200
109.967370	3353.216899	23.424218
110.193260	3354.439517	23.429235
110.005985	3363.671944	23.434253
110.270622	3357.845264	23.439271
110.246799	3355.078478	23.444288
110.047430	3360.312477	23.449306
110.399630	3357.659438	23.454323
110.582762	3364.036145	23.459341
110.746104	3385.090165	23.464359
111.113926	3390.658661	23.469376
110.638544	3388.701358	23.474394
111.142392	3377.906576	23.479411
111.042384	3391.716802	23.484429
111.096297	3405.736228	23.489447
111.270326	3411.876247	23.494464
111.150868	3419.758354	23.499482
111.486259	3421.531808	23.504499
111.740421	3419.142262	23.509517
111.831613	3438.863269	23.514535
112.381168	3443.963851	23.519552
112.090318	3444.940496	23.524570
112.596010	3445.389549	23.529587
112.515470	3442.138775	23.534605
112.332108	3447.351647	23.539623
112.370305	3444.368254	23.544640
112.034788	3454.984880	23.549658
112.587762	3463.196674	23.554675
112.776498	3464.592794	23.559693
112.903932	3473.409360	23.564711
113.192670	3465.513847	23.569728
113.274205	3486.792989	23.574746
114.113433	3489.564262	23.579763
113.616574	3483.780925	23.584781
113.378569	3490.148659	23.589799
113.825305	3477.566601	23.594816
114.023266	3495.281977	23.599834
114.036685	3485.196345	23.604851
114.065147	3476.235917	23.609869
114.057821	3486.420625	23.614887
114.425941	3481.662719	23.619904
114.631910	3489.478383	23.624922
114.710589	3507.113904	23.629939
114.670961	3512.029346	23.634957
114.729768	3519.275225	23.639975
115.153006	3511.368446	23.644992
114.976742	3516.347067	23.650010
115.111253	3509.021619	23.655027
115.418997	3511.876953	23.660045
115.259546	3507.963167	23.665063
115.415440	3497.896855	23.670080
115.378046	3521.431035	23.675098
115.616944	3525.277019	23.680115
115.597078	3533.734497	23.685133
115.800100	3532.624024	23.690151
115.788366	3524.614036	23.695168
115.714237	3536.201733	23.700186
115.752784	3553.735277	23.705203
115.967848	3564.993980	23.710221
116.150377	3561.770108	23.715239
116.341656	3561.232512	23.720256
116.100582	3573.840123	23.725274
116.449013	3586.803348	23.730291
116.716748	3581.081598	23.735309
116.700154	3588.406930	23.740327
117.218385	3598.896873	23.745344
117.127584	3614.379205	23.750362
117.413045	3611.140250	23.755379
117.659006	3608.115735	23.760397
117.578499	3615.333930	23.765415
117.968866	3609.407985	23.770432
117.964266	3610.041541	23.775450
117.755569	3612.494148	23.780467
118.076689	3611.673211	23.785485
117.795363	3629.457461	23.790503
117.972466	3632.543528	23.795520
118.091220	3644.630933	23.800538
118.188684	3637.635615	23.805555
118.511533	3659.069946	23.810573
118.748823	3673.331727	23.815591
118.807249	3671.589196	23.820608
118.456445	3662.297308	23.825626
119.159819	3678.331770	23.830643
119.150750	3692.751694	23.835661
118.893091	3703.693436	23.840679
119.718194	3694.105256	23.845696
119.520112	3689.719806	23.850714
119.613030	3693.121043	23.855731
119.938370	3700.261847	23.860749
119.892970	3712.007931	23.865767
120.261434	3721.735642	23.870784
120.657085	3720.570034	23.875802
120.456016	3723.578554	23.880819
120.541096	3717.807063	23.885837
120.426445	3710.425516	23.890855
120.577489	3706.757950	23.895872
120.761793	3731.147588	23.900890
120.747590	3733.256160	23.905907
121.216885	3735.315004	23.910925
121.099779	3741.219064	23.915943
121.167711	3738.469700	23.920960
121.334485	3748.920282	23.925978
121.336080	3754.199103	23.930995
121.873694	3755.753660	23.936013
121.901066	3767.897634	23.941031
122.039934	3754.617407	23.946048
121.907235	3765.968875	23.951066
122.011289	3763.341891	23.956083
122.230677	3779.542818	23.961101
122.138266	3796.502566	23.966119
122.471240	3785.068384	23.971136
122.254710	3791.407484	23.976154
122.431005	3794.770132	23.981171
122.862595	3821.754760	23.986189
122.991215	3828.467499	23.991207
123.210865	3822.907187	23.996224
123.238170	3818.570223	24.001242
123.237363	3813.137371	24.006259
123.524568	3842.032416	24.011277
123.181394	3845.082598	24.016295
123.856666	3840.582831	24.021312
124.042502	3845.435456	24.026330
124.055707	3841.733585	24.031347
123.926702	3835.048545	24.036365
124.176533	3854.877295	24.041383
124.522194	3870.149410	24.046400
124.432248	3861.687566	24.051418
124.444798	3865.356119	24.056435
124.814020	3869.168799	24.061453
124.505569	3874.137524	24.066471
125.148942	3868.227084	24.071488
124.670583	3872.951065	24.076506
124.958865	3889.374985	24.081523
125.358148	3882.722558	24.086541
125.462987	3891.665953	24.091559
125.882364	3885.503180	24.096576
125.377273	3893.414326	24.101594
125.478502	3887.097897	24.106611
126.060927	3908.478963	24.111629
125.936975	3917.734701	24.116647
126.062722	3909.989197	24.121664
126.126457	3915.514907	24.126682
126.114362	3921.762724	24.131699
126.563495	3931.751267	24.136717
126.769487	3940.512172	24.141735
126.659657	3940.169319	24.146752
126.951752	3935.832979	24.151770
126.615912	3943.068396	24.156787
127.218163	3955.465028	24.161805
126.991712	3976.189438	24.166823
127.432752	3972.610433	24.171840
127.677222	3959.749621	24.176858
127.392576	3975.204945	24.181875
127.935043	3975.495544	24.186893
127.474019	3981.369612	24.191911
128.178243	3975.126177	24.196928
128.223167	3974.391900	24.201946
128.213209	3994.624127	24.206963
128.553023	4005.056076	24.211981
128.616208	4012.373516	24.216999
128.725269	4003.440787	24.222016
129.079472	4005.785692	24.227034
128.994970	4009.163214	24.232051
129.393797	4019.160929	24.237069
129.200045	4021.592618	24.242087
129.439054	4029.446396	24.247104
129.201008	4032.016148	24.252122
129.594283	4035.757949	24.257139
129.899522	4041.491789	24.262157
129.932078	4055.990996	24.267175
130.074014	4061.034449	24.272192
130.074051	4065.165820	24.277210
130.245380	4075.744626	24.282227
130.761161	4058.757482	24.287245
130.502604	4070.076849	24.292263
130.658181	4079.328142	24.297280
130.966413	4083.720352	24.302298
130.969340	4088.256825	24.307315
130.859502	4083.138826	24.312333
130.857812	4091.163214	24.317351
130.973567	4103.983080	24.322368
131.643422	4113.477647	24.327386
131.458028	4116.635638	24.332403
131.765237	4111.418659	24.337421
131.486085	4122.047664	24.342439
131.852676	4136.566458	24.347456
132.124983	4139.582526	24.352474
132.114316	4146.217658	24.357491
132.206531	4141.445776	24.362509
132.400417	4161.225506	24.367527
132.406018	4170.320550	24.372544
132.790035	4173.749695	24.377562
132.798081	4173.401103	24.382579
133.222372	4170.346170	24.387597
133.055476	4188.210547	24.392615
133.244772	4190.388262	24.397632
133.289991	4197.821380	24.402650
133.616687	4196.251341	24.407667
133.963134	4191.865769	24.412685
133.553598	4200.709036	24.417703
133.911787	4199.262937	24.422720
134.092213	4222.217924	24.427738
134.400092	4225.558882	24.432755
134.097143	4218.658342	24.437773
134.662329	4219.323201	24.442791
134.424916	4226.024258	24.447808
134.745090	4222.540023	24.452826
134.969575	4236.465014	24.457843
135.080487	4241.638091	24.462861
135.041548	4246.459539	24.467879
135.568104	4241.714160	24.472896
135.374160	4233.422113	24.477914
135.083239	4238.910575	24.482931
135.682537	4261.569464	24.487949
135.798018	4279.912478	24.492967
135.960819	4272.485125	24.497984
136.147858	4268.998508	24.503002
136.180729	4284.936696	24.508019
136.584126	4289.153340	24.513037
136.447758	4298.712194	24.518055
136.516491	4297.947185	24.523072
136.714260	4293.352303	24.528090
136.724001	4299.365908	24.533107
137.153352	4320.553555	24.538125
136.985508	4318.161289	24.543143
136.834913	4328.224963	24.548160
137.363946	4327.229389	24.553178
137.704865	4345.104376	24.558195
138.330951	4350.313479	24.563213
138.060798	4352.075072	24.568231
138.213940	4350.833802	24.573248
138.220663	4345.314465	24.578266
138.014718	4359.824300	24.583283
138.384181	4361.084658	24.588301
138.767349	4375.389870	24.593319
138.921419	4372.744267	24.598336
139.064165	4377.048977	24.603354
138.994908	4377.892122	24.608371
139.076629	4373.237675	24.613389
139.231860	4386.533998	24.618407
139.589473	4399.215622	24.623424
139.685403	4392.009556	24.628442
139.956415	4392.541206	24.633459
139.748295	4392.005523	24.638477
139.660098	4404.161642	24.643495
139.491283	4418.226724	24.648512
140.105083	4426.273029	24.653530
140.143123	4438.207452	24.658547
140.350730	4440.083693	24.663565
140.745617	4452.266977	24.668583
140.353444	4458.061305	24.673600
140.582741	4451.152874	24.678618
140.664341	4477.142453	24.683635
141.318542	4482.028779	24.688653
141.264348	4480.778510	24.693671
141.188181	4487.145840	24.698688
141.848907	4498.576361	24.703706
141.494596	4502.974423	24.708723
141.852569	4515.276486	24.713741
142.101995	4523.004356	24.718759
142.038403	4533.920057	24.723776
142.727393	4525.654153	24.728794
142.386220	4535.021031	24.733811
142.638897	4537.187515	24.738829
143.121924	4529.059664	24.743847
143.147970	4532.534764	24.748864
143.147758	4524.445178	24.753882
143.414238	4528.344337	24.758899
143.257119	4545.254571	24.763917
143.659945	4547.971107	24.768935
143.631714	4549.961223	24.773952
143.703284	4548.889377	24.778970
143.503197	4547.019831	24.783987
143.764246	4560.264130	24.789005
144.438602	4570.832447	24.794023
144.575886	4581.827544	24.799040
144.629780	4582.021848	24.804058
144.697232	4584.797851	24.809075
145.122432	4584.716470	24.814093
144.944655	4576.630265	24.819111
144.827328	4601.184995	24.824128
144.981571	4607.215747	24.829146
144.838330	4618.884989	24.834163
145.305980	4616.682011	24.839181
145.126716	4631.261707	24.844199
145.411919	4646.187437	24.849216
145.840802	4641.166717	24.854234
146.058595	4670.678046	24.859251
146.458857	4666.765417	24.864269
146.749335	4671.149708	24.869287
146.583778	4664.001772	24.874304
146.828407	4662.104265	24.879322
146.772770	4671.649192	24.884339
146.904633	4684.959874	24.889357
147.289928	4686.024689	24.894375
147.118311	4693.479764	24.899392
147.675076	4671.725996	24.904410
147.789918	4681.163162	24.909427
147.930542	4691.248160	24.914445
147.847647	4694.408985	24.919463
148.227117	4703.665321	24.924480
148.190124	4698.994204	24.929498
148.177792	4710.544184	24.934515
148.368583	4720.849286	24.939533
148.928800	4738.685267	24.944551
148.817806	4742.954906	24.949568
148.756576	4740.400802	24.954586
149.054236	4740.609093	24.959603
149.058860	4742.894640	24.964621
149.578108	4756.145188	24.969639
149.493785	4767.847313	24.974656
149.902131	4772.270399	24.979674
149.772291	4773.994632	24.984691
149.392234	4774.159187	24.989709
149.753498	4791.547755	24.994727
149.960474	4810.983549	24.999744
150.241192	4805.287955	25.004762
150.547116	4818.336029	25.009779
150.543441	4822.509954	25.014797
150.639236	4812.807155	25.019815
150.415504	4825.219942	25.024832
150.982353	4833.975160	25.029850
151.327281	4836.888773	25.034867
151.387655	4845.289963	25.039885
152.079381	4855.103477	25.044903
151.933917	4871.567160	25.049920
152.377505	4861.516929	25.054938
152.158566	4868.099427	25.059955
151.885642	4872.909400	25.064973
152.202475	4862.417067	25.069991
152.291354	4880.576173	25.075008
152.656710	4891.137585	25.080026
152.384884	4896.675091	25.085043
152.464463	4904.525777	25.090061
153.089772	4898.875484	25.095079
153.150218	4917.853681	25.100096
153.674405	4916.465096	25.105114
153.387284	4928.269432	25.110131
153.722755	4915.376632	25.115149
153.953820	4910.761883	25.120167
154.113793	4928.378456	25.125184
154.363365	4937.348497	25.130202
154.746161	4941.587633	25.135219
154.615385	4927.819845	25.140237
154.745158	4937.768186	25.145255
154.946146	4934.069623	25.150272
154.953858	4927.370933	25.155290
155.072787	4926.478661	25.160307
155.216412	4942.232216	25.165325
155.463999	4953.893707	25.170343
155.402888	4965.986708	25.175360
155.313547	4968.383140	25.180378
155.649310	4977.860305	25.185395
156.050747	4987.192716	25.190413
156.163046	4983.268616	25.195431
156.420633	5003.065639	25.200448
156.468641	5000.542237	25.205466
156.735371	5009.995409	25.210483
156.753274	5017.200317	25.215501
157.099449	5003.570871	25.220519
157.275290	5013.896755	25.225536
157.198870	5022.389992	25.230554
157.336866	5031.206869	25.235571
157.524749	5039.873729	25.240589
157.843586	5040.555000	25.245607
157.857948	5060.780635	25.250624
157.840791	5058.109709	25.255642
158.120389	5063.539445	25.260659
158.241250	5069.929522	25.265677
158.519776	5075.550032	25.270695
158.787832	5095.280857	25.275712
158.893814	5099.494982	25.280730
159.264085	5093.699402	25.285747
158.911809	5099.265261	25.290765
159.318781	5104.369921	25.295783
159.224222	5121.208196	25.300800
159.575776	5121.604466	25.305818
159.848129	5138.016582	25.310835
160.117093	5149.835346	25.315853
160.158559	5144.944763	25.320871
160.160742	5151.247410	25.325888
160.490192	5150.369104	25.330906
160.619043	5162.678893	25.335923
160.758864	5169.371452	25.340941
160.797957	5166.640791	25.345959
160.966698	5179.596103	25.350976
161.639882	5190.132746	25.355994
161.662625	5190.803975	25.361011
161.778680	5198.897644	25.366029
162.245329	5197.485483	25.371047
161.891194	5201.233955	25.376064
162.114713	5202.486257	25.381082
162.127956	5210.054311	25.386099
162.213571	5222.961989	25.391117
162.426423	5224.429492	25.396135
162.449811	5239.751967	25.401152
162.695289	5244.896798	25.406170
162.922370	5254.630760	25.411187
162.993174	5257.123586	25.416205
163.059608	5256.030490	25.421223
163.196451	5273.300806	25.426240
163.391505	5278.609149	25.431258
163.166039	5286.925582	25.436275
163.422140	5305.801760	25.441293
163.610730	5304.955429	25.446311
163.813592	5321.081534	25.451328
164.196225	5335.809859	25.456346
164.317398	5338.384144	25.461363
164.325119	5354.319703	25.466381
164.884501	5358.033540	25.471399
165.339765	5367.823519	25.476416
165.306213	5372.608191	25.481434
165.720813	5372.557707	25.486451
165.483000	5388.093687	25.491469
166.127973	5384.942137	25.496487
165.805439	5387.688334	25.501504
166.091660	5384.060616	25.506522
166.558053	5401.237922	25.511539
166.306424	5421.597052	25.516557
166.657054	5417.673556	25.521575
167.018833	5418.711602	25.526592
167.267427	5418.984735	25.531610
167.156694	5425.712581	25.536627
166.968126	5443.030653	25.541645
167.515768	5442.055566	25.546663
167.206271	5446.896182	25.551680
167.403174	5456.109154	25.556698
168.194365	5466.524849	25.561715
168.118665	5472.166340	25.566733
168.181589	5474.161959	25.571751
168.230668	5490.117586	25.576768
168.381946	5496.687886	25.581786
168.894195	5510.905822	25.586803
168.642167	5525.324330	25.591821
168.852893	5535.925953	25.596839
169.233569	5545.183376	25.601856
169.218750	5547.580160	25.606874
169.777746	5546.480323	25.611891
169.601368	5556.170213	25.616909
170.199973	5560.135151	25.621927
170.532144	5574.462504	25.626944
170.554886	5581.516437	25.631962
170.864180	5578.830760	25.636979
170.640776	5582.572642	25.641997
170.816710	5582.412815	25.647015
170.839824	5609.956849	25.652032
170.903150	5614.375074	25.657050
170.917196	5614.826445	25.662067
171.240114	5634.883595	25.667085
171.482901	5644.125311	25.672103
171.551520	5647.701511	25.677120
171.755697	5663.766317	25.682138
172.080628	5664.984541	25.687156
172.377202	5683.329142	25.692173
173.095031	5690.891047	25.697191
173.050814	5694.286674	25.702208
172.782498	5689.032928	25.707226
173.403310	5682.655363	25.712244
173.363790	5687.705752	25.717261
173.230169	5699.119014	25.722279
173.282229	5712.155514	25.727296
173.517589	5714.153334	25.732314
173.926050	5734.442181	25.737332
174.368504	5745.018185	25.742349
174.703296	5732.579282	25.747367
174.305764	5739.674508	25.752384
174.482602	5748.038785	25.757402
175.149946	5747.251005	25.762420
175.043339	5761.596823	25.767437
175.448310	5761.977969	25.772455
175.471410	5769.925073	25.777472
175.561787	5769.249348	25.782490
175.842895	5759.994942	25.787508
175.402309	5780.800096	25.792525
175.673125	5794.636888	25.797543
175.965365	5802.492197	25.802560
176.157830	5810.630239	25.807578
176.426974	5818.228680	25.812596
176.480255	5826.545719	25.817613
176.661228	5822.907759	25.822631
177.040861	5855.942699	25.827648
177.400775	5851.545781	25.832666
177.565920	5845.093941	25.837684
177.505468	5865.588965	25.842701
177.898190	5881.188805	25.847719
177.834364	5883.348805	25.852736
177.752731	5888.084884	25.857754
178.289170	5890.260504	25.862772
178.173668	5909.465925	25.867789
178.522852	5913.832972	25.872807
178.429631	5924.960894	25.877824
178.626450	5940.064735	25.882842
179.039570	5939.755373	25.887860
178.978618	5966.431029	25.892877
179.313499	5965.993635	25.897895
179.495706	5982.023809	25.902912
179.698978	5995.327716	25.907930
180.066837	5994.214600	25.912948
180.036575	6012.671975	25.917965
180.260465	6022.332905	25.922983
180.884897	6022.634408	25.928000
180.833258	6037.591232	25.933018
181.269581	6043.926331	25.938036
181.117102	6056.627582	25.943053
180.932270	6060.446677	25.948071
181.570925	6078.123126	25.953088
181.602008	6090.566393	25.958106
182.004931	6095.989461	25.963124
182.188127	6099.040355	25.968141
182.114056	6105.075613	25.973159
182.797390	6109.776484	25.978176
182.788275	6120.598411	25.983194
182.877914	6109.879801	25.988212
182.858379	6140.955650	25.993229
182.862175	6144.497012	25.998247
183.365149	6146.199333	26.003264
183.409197	6161.809916	26.008282
183.981913	6168.387128	26.013300
183.850777	6168.685333	26.018317
184.097647	6173.046551	26.023335
184.086514	6180.065403	26.028352
184.331666	6188.943952	26.033370
184.871363	6210.941318	26.038388
184.886938	6216.256062	26.043405
185.229784	6223.547137	26.048423
185.540251	6215.137459	26.053440
185.490970	6221.255296	26.058458
186.052470	6232.396342	26.063476
185.807728	6249.296124	26.068493
186.177273	6252.507592	26.073511
186.387858	6242.620299	26.078528
186.157095	6247.909673	26.083546
186.543976	6269.042395	26.088564
186.611287	6277.003702	26.093581
186.624927	6274.243196	26.098599
187.100693	6275.712959	26.103616
187.140437	6296.889008	26.108634
187.663241	6300.948601	26.113652
187.491001	6304.978331	26.118669
187.632023	6300.795533	26.123687
187.933078	6305.694435	26.128704
188.328336	6330.890043	26.133722
188.602385	6328.057276	26.138740
188.335347	6339.492298	26.143757
188.369268	6350.828673	26.148775
188.723978	6355.628917	26.153792
188.467895	6370.085095	26.158810
188.952989	6379.922754	26.163828
189.101959	6391.932445	26.168845
189.065126	6411.251472	26.173863
189.480931	6421.591327	26.178880
189.873085	6439.530315	26.183898
190.054965	6443.792097	26.188916
190.213428	6454.182451	26.193933
190.453061	6477.816172	26.198951
190.727548	6479.908433	26.203968
190.703717	6485.269960	26.208986
191.296112	6500.194642	26.214004
191.616260	6508.718332	26.219021
191.719419	6506.873961	26.224039
192.066791	6520.252123	26.229056
191.904240	6531.609337	26.234074
192.148109	6533.674380	26.239092
192.276025	6536.752626	26.244109
192.577546	6546.861011	26.249127
192.877933	6552.787191	26.254144
192.818115	6557.001586	26.259162
193.179775	6564.207003	26.264180
193.158449	6577.897509	26.269197
193.304350	6593.605865	26.274215
193.554673	6590.523357	26.279232
193.783760	6613.075223	26.284250
194.069625	6614.526835	26.289268
194.436110	6619.691469	26.294285
194.308401	6647.805754	26.299303
194.928186	6640.552115	26.304320
194.608966	6656.538382	26.309338
194.981556	6667.290404	26.314356
195.431166	6664.080374	26.319373
195.705158	6666.296403	26.324391
195.795702	6684.366727	26.329408
195.957495	6698.175102	26.334426
196.435612	6702.503699	26.339444
196.310672	6703.768913	26.344461
196.013585	6718.121923	26.349479
196.542245	6729.939841	26.354496
196.600234	6739.748398	26.359514
197.084062	6755.369466	26.364532
197.273922	6761.429807	26.369549
197.288457	6761.143884	26.374567
197.686545	6780.490607	26.379584
197.596698	6800.051242	26.384602
197.845876	6795.840959	26.389620
198.178058	6818.055473	26.394637
198.117012	6821.096530	26.399655
198.303654	6826.611581	26.404672
198.364551	6850.839411	26.409690
198.958632	6852.882754	26.414708
199.138332	6873.543329	26.419725
198.918491	6884.590488	26.424743
199.504768	6889.688107	26.429760
199.619285	6915.149303	26.434778
200.085099	6919.790337	26.439796
200.176311	6916.432431	26.444813
199.892107	6927.048395	26.449831
200.328933	6934.613316	26.454848
200.702342	6936.326937	26.459866
201.037647	6947.596518	26.464884
201.354797	6952.555183	26.469901
201.207476	6968.103719	26.474919
201.539914	6964.257688	26.479936
201.985413	6991.071774	26.484954
201.755849	6992.119606	26.489972
202.121240	7001.997162	26.494989
202.538178	7010.031712	26.500007
202.758241	7018.678581	26.505024
202.714387	7022.150049	26.510042
202.755156	7029.975922	26.515060
203.309075	7042.322358	26.520077
203.097419	7051.491259	26.525095
203.671010	7060.356888	26.530112
203.634734	7081.541055	26.535130
203.658788	7085.019411	26.540148
204.183478	7088.054925	26.545165
204.136893	7106.831343	26.550183
204.428219	7106.735895	26.555200
204.759537	7121.984799	26.560218
204.734725	7123.884877	26.565236
205.037152	7139.675774	26.570253
205.362311	7160.270896	26.575271
205.450825	7164.196238	26.580288
205.392188	7181.610484	26.585306
205.861431	7199.426512	26.590324
205.956778	7200.656874	26.595341
206.155902	7231.624619	26.600359
206.564699	7236.533545	26.605376
206.878033	7248.726199	26.610394
206.908054	7266.298364	26.615412
207.155009	7271.060015	26.620429
207.504008	7291.275636	26.625447
207.757350	7279.821800	26.630464
207.639083	7300.477118	26.635482
208.125457	7312.608094	26.640500
208.544739	7318.071415	26.645517
208.166130	7336.098054	26.650535
208.528119	7349.398881	26.655552
208.973406	7365.556258	26.660570
209.174504	7377.265835	26.665588
209.575760	7385.475676	26.670605
209.455253	7392.772319	26.675623
209.908283	7399.115441	26.680640
210.092626	7409.251653	26.685658
210.339355	7408.939884	26.690676
210.481184	7425.100295	26.695693
210.424251	7448.864901	26.700711
210.846749	7440.369869	26.705728
211.106456	7467.778715	26.710746
210.908775	7470.434490	26.715764
211.755882	7483.395973	26.720781
211.541654	7503.464068	26.725799
212.235256	7486.091736	26.730816
212.196860	7510.964012	26.735834
212.414153	7519.999158	26.740852
212.462336	7525.210481	26.745869
212.389006	7534.411111	26.750887
213.088061	7548.666133	26.755904
213.041279	7557.368497	26.760922
212.834171	7577.655274	26.765940
213.582059	7591.473743	26.770957
213.770560	7591.964821	26.775975
214.032424	7602.710604	26.780992
213.884200	7626.311780	26.786010
214.059039	7620.062419	26.791028
214.262828	7643.339894	26.796045
214.598395	7656.967522	26.801063
214.438354	7673.104900	26.806080
215.074464	7681.914056	26.811098
215.180144	7687.918582	26.816116
215.054124	7717.122292	26.821133
215.263667	7731.683794	26.826151
215.311720	7739.964892	26.831168
215.847283	7760.246327	26.836186
215.942381	7766.489734	26.841204
216.132771	7790.128046	26.846221
216.331693	7811.529466	26.851239
216.686808	7828.890894	26.856256
217.430983	7841.820086	26.861274
217.685841	7857.128041	26.866292
217.949247	7867.144328	26.871309
218.138158	7881.061885	26.876327
218.359036	7892.016303	26.881344
218.443857	7899.792775	26.886362
218.472605	7914.191383	26.891380
218.980577	7914.230218	26.896397
219.349653	7932.942739	26.901415
219.970446	7941.055874	26.906432
220.017768	7951.564859	26.911450
220.092406	7959.615596	26.916468
220.645228	7959.353976	26.921485
220.343810	7961.218807	26.926503
221.077761	7972.431005	26.931520
220.918840	7972.663733	26.936538
221.215066	7982.898372	26.941556
221.399877	7985.164800	26.946573
221.486209	8004.694598	26.951591
221.482344	8009.794174	26.956608
221.916645	8020.314766	26.961626
221.630242	8031.016110	26.966644
222.058320	8037.723609	26.971661
222.168210	8062.564321	26.976679
222.772161	8063.344268	26.981696
223.023644	8087.449480	26.986714
223.058493	8100.902769	26.991732
223.544356	8107.974113	26.996749
223.494075	8130.111985	27.001767
223.543401	8131.202734	27.006784
223.816737	8153.151579	27.011802
224.132728	8162.486631	27.016820
224.675216	8178.223067	27.021837
224.416074	8195.158800	27.026855
225.114054	8200.590473	27.031872
225.330219	8210.403687	27.036890
225.260281	8226.264393	27.041908
225.798752	8228.307678	27.046925
225.438472	8251.213866	27.051943
225.930825	8260.589102	27.056960
226.279619	8280.221520	27.061978
226.383039	8292.053496	27.066996
226.697201	8303.849021	27.072013
226.816059	8316.223571	27.077031
227.352428	8327.682991	27.082048
227.325842	8340.403819	27.087066
227.213452	8362.666515	27.092084
227.435477	8369.187699	27.097101
227.964959	8383.266733	27.102119
228.503658	8403.009659	27.107136
228.321760	8404.376599	27.112154
228.365755	8415.462276	27.117172
228.961994	8430.834008	27.122189
229.198949	8440.587204	27.127207
229.404714	8449.093064	27.132224
229.606819	8455.167781	27.137242
229.773216	8470.350751	27.142260
230.354108	8484.569460	27.147277
230.312565	8492.987092	27.152295
230.675751	8488.751981	27.157312
230.792308	8505.416311	27.162330
230.869100	8514.518607	27.167348
230.919737	8526.392580	27.172365
231.278311	8545.263534	27.177383
231.365854	8553.393571	27.182400
231.770703	8571.242281	27.187418
231.896061	8592.124410	27.192436
232.006427	8602.852622	27.197453
232.546310	8628.799141	27.202471
232.919135	8644.910735	27.207488
233.037295	8645.586009	27.212506
233.138452	8673.141336	27.217524
233.384703	8679.190713	27.222541
233.487516	8701.523027	27.227559
233.913700	8710.350179	27.232576
234.488999	8726.525233	27.237594
234.495920	8743.842889	27.242612
234.653654	8744.555731	27.247629
234.990812	8769.879051	27.252647
235.333389	8774.227511	27.257664
235.357486	8787.701276	27.262682
235.570171	8804.243658	27.267700
235.952869	8812.109123	27.272717
236.341527	8829.455062	27.277735
236.642629	8838.089508	27.282752
236.797977	8856.940115	27.287770
236.774356	8877.452610	27.292788
237.385113	8876.459016	27.297805
237.841992	8891.448566	27.302823
237.744061	8902.804644	27.307840
238.079445	8905.136085	27.312858
238.024729	8924.732106	27.317876
238.521571	8929.438713	27.322893
238.529837	8949.187406	27.327911
238.943951	8962.759037	27.332928
239.330541	8963.303237	27.337946
239.441056	8988.175218	27.342964
239.381462	8986.281092	27.347981
239.826637	9003.693490	27.352999
240.303473	9017.020030	27.358016
240.314680	9016.994582	27.363034
240.719385	9036.371317	27.368052
240.805745	9048.535964	27.373069
240.981512	9060.071361	27.378087
240.976428	9076.910825	27.383104
241.411540	9088.515176	27.388122
241.403235	9109.278307	27.393140
241.500394	9117.688275	27.398157
241.845608	9129.391040	27.403175
242.128159	9151.468139	27.408192
242.445567	9169.560446	27.413210
242.790897	9190.187154	27.418228
242.957525	9198.179172	27.423245
243.553232	9219.385240	27.428263
243.607820	9231.660848	27.433280
243.649823	9236.039496	27.438298
244.193668	9261.626374	27.443316
244.466747	9257.210610	27.448333
244.376317	9283.045891	27.453351
244.614353	9294.706648	27.458368
245.263855	9302.231199	27.463386
245.313415	9324.521204	27.468404
245.654646	9321.846170	27.473421
246.116963	9327.037583	27.478439
246.076176	9350.899238	27.483456
246.473167	9352.145223	27.488474
246.512621	9375.385463	27.493492
246.842477	9376.544877	27.498509
246.914033	9389.604008	27.503527
246.892089	9419.701910	27.508544
247.439147	9408.843134	27.513562
247.221948	9437.815345	27.518580
247.635096	9443.947677	27.523597
247.933207	9473.580687	27.528615
248.025575	9495.638535	27.533632
248.295323	9503.779860	27.538650
248.660025	9526.510349	27.543668
248.743122	9538.361580	27.548685
249.035233	9568.790642	27.553703
249.354270	9578.372601	27.558720
249.765560	9598.498120	27.563738
249.572339	9627.200427	27.568756
250.248729	9638.378431	27.573773
250.874475	9655.760075	27.578791
250.601421	9678.556169	27.583808
251.321752	9689.548105	27.588826
251.687001	9709.226036	27.593844
251.674518	9708.872056	27.598861
252.063007	9733.552648	27.603879
252.301827	9735.425152	27.608896
252.533667	9756.651199	27.613914
252.964436	9768.179559	27.618932
253.196705	9789.714397	27.623949
253.468794	9794.162252	27.628967
253.768505	9799.207420	27.633984
253.979663	9820.176210	27.639002
254.369983	9821.346133	27.644020
254.287058	9836.281756	27.649037
254.632393	9852.631522	27.654055
254.833033	9869.748947	27.659072
255.464328	9881.463995	27.664090
255.399067	9893.892300	27.669108
255.815083	9915.816795	27.674125
255.805577	9924.676563	27.679143
256.070649	9940.879778	27.684160
256.218207	9953.530516	27.689178
256.605400	9969.339335	27.694196
257.052138	9980.787212	27.699213
257.194291	9986.947279	27.704231
256.912363	10011.204346	27.709248
257.634342	10019.421550	27.714266
257.482485	10048.792919	27.719284
257.995936	10063.372419	27.724301
258.295330	10071.783287	27.729319
258.452018	10100.125993	27.734336
259.111485	10092.317505	27.739354
259.135116	10133.952343	27.744372
259.579619	10134.275079	27.749389
259.806740	10153.091695	27.754407
259.836241	10172.587060	27.759424
260.321402	10176.898911	27.764442
260.507151	10199.036806	27.769460
260.842738	10205.279961	27.774477
260.800367	10217.654306	27.779495
260.888963	10238.896822	27.784512
261.379558	10255.725588	27.789530
261.806866	10277.322547	27.794548
261.916160	10295.293008	27.799565
262.333511	10302.453882	27.804583
262.558711	10318.283557	27.809600
262.943350	10328.889529	27.814618
262.716711	10342.452583	27.819636
263.127938	10349.320631	27.824653
263.547327	10362.813795	27.829671
263.916043	10388.932525	27.834688
264.336828	10385.471285	27.839706
264.145257	10413.086718	27.844724
264.408243	10428.801526	27.849741
264.976076	10426.289703	27.854759
264.684120	10448.644885	27.859776
265.230882	10466.250837	27.864794
265.339202	10484.264214	27.869812
265.629144	10505.580112	27.874829
265.964830	10512.967315	27.879847
265.815618	10544.863391	27.884864
266.543219	10563.933265	27.889882
266.795760	10593.085845	27.894900
266.983856	10613.274005	27.899917
267.516179	10620.850094	27.904935
267.463534	10647.831563	27.909952
267.935689	10656.402438	27.914970
268.198154	10672.596581	27.919988
268.341025	10696.197413	27.925005
268.847815	10713.419479	27.930023
269.225143	10745.020801	27.935040
269.598185	10744.814127	27.940058
269.787805	10753.921865	27.945076
269.753104	10774.939686	27.950093
270.150533	10786.461693	27.955111
270.419550	10814.918635	27.960128
270.716200	10826.564501	27.965146
270.895187	10846.836398	27.970164
270.887148	10870.229258	27.975181
271.894463	10884.149470	27.980199
272.239356	10906.651985	27.985216
272.091201	10911.723578	27.990234
272.651296	10930.870463	27.995252
272.856750	10936.899875	28.000269
273.353353	10950.427236	28.005287
273.431324	10967.990005	28.010304
273.928890	10976.069946	28.015322
274.120542	10992.640125	28.020340
273.981498	11002.577664	28.025357
274.782688	11016.179147	28.030375
274.627625	11035.223930	28.035392
274.880874	11048.641961	28.040410
275.084794	11055.402811	28.045428
275.373244	11087.944473	28.050445
275.654735	11099.589894	28.055463
276.095767	11124.549134	28.060480
276.318885	11143.562961	28.065498
276.372119	11164.453279	28.070516
276.790888	11182.928953	28.075533
277.204106	11193.217981	28.080551
277.637846	11219.976504	28.085568
277.608338	11228.655935	28.090586
277.928667	11251.846873	28.095604
278.154866	11266.993437	28.100621
278.642499	11269.238576	28.105639
278.895352	11292.361953	28.110656
279.041751	11309.195221	28.115674
279.456353	11312.448334	28.120692
279.706145	11332.710697	28.125709
280.184385	11351.587995	28.130727
280.211757	11366.496532	28.135744
280.499982	11380.561417	28.140762
280.806009	11392.392081	28.145780
280.738699	11414.933594	28.150797
281.059558	11417.858728	28.155815
280.920851	11446.909002	28.160832
281.419255	11459.659638	28.165850
281.906388	11472.093845	28.170868
281.999215	11500.511824	28.175885
282.430008	11511.326032	28.180903
282.689643	11532.004597	28.185920
283.336262	11549.234354	28.190938
283.734872	11572.582980	28.195956
283.632488	11574.367996	28.200973
284.130248	11581.244312	28.205991
284.298593	11598.510740	28.211008
284.279182	11629.878488	28.216026
284.490602	11648.437867	28.221044
284.667858	11666.249692	28.226061
285.441537	11681.711004	28.231079
285.612505	11708.732866	28.236096
285.520533	11731.449087	28.241114
286.084953	11755.287394	28.246132
286.404654	11774.508165	28.251149
286.631891	11789.697594	28.256167
286.885305	11824.919104	28.261184
287.311176	11839.699084	28.266202
287.861252	11861.336939	28.271220
287.839472	11878.576830	28.276237
288.285061	11892.375014	28.281255
288.668223	11914.089417	28.286272
288.967393	11939.684815	28.291290
289.379589	11949.813763	28.296308
289.426529	11976.897572	28.301325
289.875966	11996.043554	28.306343
290.057251	12001.696016	28.311360
290.687531	12007.652359	28.316378
290.422384	12035.452922	28.321396
291.147713	12057.652968	28.326413
291.679724	12074.919592	28.331431
291.781277	12091.723275	28.336448
291.867472	12105.139894	28.341466
292.266764	12112.964056	28.346484
292.433801	12155.211481	28.351501
292.753143	12153.445724	28.356519
292.856444	12179.893358	28.361536
293.155663	12201.595252	28.366554
293.348081	12217.359726	28.371572
293.699076	12246.968593	28.376589
293.999139	12263.244780	28.381607
294.318303	12286.336539	28.386624
294.768415	12308.472174	28.391642
295.489400	12319.566671	28.396660
295.466794	12352.102476	28.401677
296.228999	12358.210460	28.406695
296.264520	12378.017929	28.411712
296.342287	12389.044018	28.416730
296.618303	12405.050127	28.421748
296.786374	12423.710544	28.426765
297.404448	12441.177632	28.431783
297.955971	12458.282273	28.436800
298.015983	12481.366777	28.441818
298.153867	12486.229200	28.446836
298.226880	12499.511225	28.451853
298.881159	12499.642502	28.456871
299.208107	12530.109991	28.461888
299.369022	12543.494117	28.466906
299.729010	12557.264489	28.471924
299.838897	12571.823237	28.476941
300.205904	12591.401176	28.481959
300.763083	12600.269467	28.486976
300.798737	12619.877071	28.491994
301.160084	12630.634187	28.497012
301.091074	12645.047687	28.502029
301.429854	12663.341309	28.507047
301.731258	12671.382083	28.512064
302.055760	12698.380180	28.517082
302.628265	12721.709560	28.522100
302.625393	12744.778055	28.527117
302.739821	12760.921574	28.532135
303.242477	12780.422132	28.537152
303.266532	12816.966541	28.542170
303.494892	12821.710079	28.547188
303.799703	12865.299703	28.552205
304.255406	12875.333780	28.557223
304.924200	12897.246490	28.562240
304.783480	12928.682523	28.567258
305.388069	12947.153096	28.572276
305.405785	12975.743679	28.577293
305.882468	12994.222869	28.582311
306.397979	13019.481584	28.587328
306.430514	13044.615408	28.592346
306.779283	13060.881181	28.597364
306.973166	13083.389653	28.602381
307.957663	13091.353819	28.607399
308.306705	13115.671039	28.612416
308.500161	13127.655560	28.617434
309.157287	13140.775239	28.622452
309.189655	13163.769153	28.627469
309.318608	13178.025859	28.632487
309.687960	13201.906462	28.637504
309.942660	13212.728895	28.642522
310.664997	13222.834099	28.647540
310.698949	13251.729788	28.652557
310.859588	13264.113827	28.657575
311.218886	13282.798737	28.662592
311.149476	13317.768028	28.667610
311.797553	13333.918344	28.672628
312.253339	13359.345068	28.677645
312.262444	13377.837472	28.682663
312.431014	13389.860976	28.687680
313.088220	13409.907208	28.692698
313.589533	13432.448804	28.697716
313.736575	13456.978051	28.702733
313.995164	13480.117780	28.707751
314.517529	13487.688996	28.712768
315.019527	13503.452332	28.717786
315.224386	13514.456572	28.722804
314.973379	13541.847605	28.727821
315.608435	13561.306700	28.732839
316.022851	13580.945751	28.737856
315.859180	13607.553361	28.742874
316.433649	13625.426092	28.747892
316.980209	13644.401923	28.752909
317.090231	13661.809427	28.757927
317.604172	13672.102277	28.762944
317.739298	13710.701150	28.767962
318.141211	13716.246773	28.772980
318.565132	13742.885004	28.777997
318.705646	13751.770886	28.783015
318.902294	13786.397702	28.788032
319.105115	13809.276056	28.793050
319.826223	13823.060228	28.798068
320.048462	13854.356013	28.803085
320.476372	13860.111719	28.808103
320.931694	13869.516074	28.813120
320.737612	13895.736760	28.818138
321.317968	13903.758768	28.823156
321.804972	13924.552467	28.828173
321.582111	13939.298319	28.833191
322.421768	13956.754007	28.838208
322.630224	13971.261441	28.843226
322.999394	13986.204062	28.848244
323.240793	14015.137685	28.853261
323.609710	14026.154516	28.858279
324.005669	14031.004632	28.863296
324.352798	14053.804283	28.868314
324.541226	14068.168549	28.873332
324.819139	14085.525076	28.878349
324.839893	14102.813862	28.883367
325.025206	14116.469472	28.888384
325.337312	14156.576734	28.893402
325.897049	14184.368928	28.898420
325.947894	14204.120915	28.903437
326.505930	14222.520266	28.908455
326.788916	14237.304017	28.913472
327.118926	14276.951558	28.918490
327.654879	14291.777020	28.923508
327.488113	14319.544692	28.928525
327.689258	14348.173508	28.933543
328.348002	14370.933058	28.938560
328.751459	14406.746824	28.943578
329.319576	14417.390522	28.948596
329.682351	14451.625604	28.953613
330.070439	14475.289050	28.958631
330.600119	14489.097592	28.963648
330.675152	14516.586014	28.968666
331.014807	14535.245665	28.973684
331.401527	14565.456467	28.978701
331.750542	14581.591328	28.983719
331.984171	14594.537987	28.988736
332.173288	14617.612020	28.993754
332.713943	14647.531138	28.998772
333.114539	14664.228085	29.003789
333.489344	14689.189579	29.008807
334.099519	14697.282698	29.013824
334.112920	14716.296010	29.018842
334.664015	14739.827261	29.023860
334.553697	14759.970668	29.028877
334.911057	14785.504166	29.033895
335.590116	14803.233215	29.038912
335.661825	14823.310322	29.043930
336.292728	14845.353288	29.048948
336.436807	14872.490441	29.053965
336.593969	14893.536979	29.058983
337.285120	14918.181678	29.064000
337.614155	14937.305344	29.069018
337.854078	14959.250836	29.074036
337.984262	14968.645020	29.079053
338.428787	14998.155139	29.084071
338.847985	15022.134177	29.089088
339.006432	15049.857137	29.094106
339.493988	15077.240394	29.099124
339.851361	15094.948925	29.104141
340.124552	15117.105050	29.109159
340.693511	15130.045492	29.114176
340.846385	15162.863610	29.119194
341.158678	15185.172545	29.124212
341.433244	15201.738014	29.129229
341.457149	15223.997012	29.134247
342.108223	15249.202067	29.139264
341.864917	15285.145285	29.144282
342.818085	15300.657583	29.149300
343.205872	15329.616581	29.154317
343.415604	15359.156752	29.159335
343.991110	15366.507273	29.164352
344.087557	15399.243784	29.169370
344.356907	15411.423894	29.174388
344.989860	15431.211834	29.179405
344.801555	15453.110648	29.184423
345.419606	15477.916447	29.189440
345.656707	15500.480983	29.194458
345.936401	15522.061279	29.199476
346.488990	15546.424081	29.204493
346.533284	15571.323406	29.209511
346.867226	15595.336306	29.214528
346.851089	15622.701387	29.219546
347.294507	15646.262795	29.224564
347.727158	15683.584492	29.229581
347.872731	15704.961831	29.234599
348.455253	15737.471981	29.239616
348.889170	15774.158471	29.244634
349.296404	15800.019443	29.249652
350.035934	15825.853830	29.254669
350.249731	15856.754476	29.259687
350.774262	15878.144977	29.264704
351.197877	15910.011883	29.269722
351.535877	15920.866456	29.274740
352.142382	15944.842637	29.279757
351.992938	15973.954731	29.284775
352.750054	15984.498821	29.289792
352.822627	16008.867672	29.294810
353.244604	16032.526178	29.299828
353.477336	16061.729644	29.304845
353.892942	16095.522794	29.309863
354.332213	16111.026344	29.314880
354.357166	16134.416547	29.319898
354.845614	16168.662778	29.324916
355.169440	16193.340239	29.329933
355.253289	16216.274738	29.334951
356.145911	16237.417214	29.339968
356.419222	16265.982256	29.344986
356.765944	16295.094762	29.350004
357.402600	16318.447035	29.355021
357.464232	16341.353859	29.360039
357.875162	16365.960418	29.365056
358.484004	16391.861459	29.370074
358.449071	16414.171205	29.375092
359.118835	16434.795980	29.380109
359.214955	16460.220841	29.385127
359.959405	16483.938539	29.390144
359.957726	16515.266990	29.395162
360.185933	16545.912762	29.400180
360.977239	16573.855101	29.405197
361.254818	16595.328389	29.410215
361.448423	16614.370809	29.415232
362.236265	16636.073378	29.420250
362.264778	16672.915657	29.425268
362.775457	16685.012634	29.430285
362.692797	16722.948444	29.435303
363.253719	16729.822807	29.440320
363.982021	16761.268928	29.445338
363.857920	16788.377955	29.450356
364.217432	16811.549811	29.455373
364.327232	16841.164342	29.460391
365.121816	16863.531289	29.465408
365.136403	16891.293762	29.470426
365.672068	16920.320928	29.475444
366.113616	16948.391144	29.480461
366.682498	16975.001169	29.485479
366.768430	17001.338073	29.490496
367.007582	17040.327915	29.495514
367.415251	17051.389235	29.500532
367.645466	17086.515551	29.505549
368.338682	17123.084884	29.510567
368.645512	17135.709317	29.515584
368.717580	17163.253080	29.520602
369.192392	17189.163368	29.525620
369.769467	17214.714709	29.530637
369.930696	17241.468294	29.535655
370.793075	17264.639527	29.540672
370.971585	17283.894868	29.545690
371.016605	17305.790616	29.550708
371.490467	17331.234688	29.555725
371.743340	17363.660728	29.560743
371.859529	17393.982966	29.565760
372.574236	17417.182007	29.570778
373.009674	17443.840092	29.575796
373.121869	17473.668163	29.580813
373.556954	17511.403436	29.585831
373.817218	17545.091267	29.590848
374.100309	17573.258127	29.595866
374.607940	17608.076382	29.600884
374.970662	17633.449459	29.605901
375.275104	17664.882324	29.610919
375.943212	17695.309238	29.615936
376.331848	17726.617939	29.620954
376.325610	17771.403878	29.625972
376.754854	17794.366944	29.630989
376.911562	17835.169370	29.636007
377.777595	17855.096628	29.641024
378.024311	17897.345621	29.646042
378.364220	17931.104601	29.651060
378.625503	17948.729633	29.656077
379.186779	17995.555115	29.661095
379.882995	18029.412966	29.666112
380.548896	18056.346022	29.671130
380.882193	18086.717140	29.676148
381.085172	18109.000821	29.681165
381.365378	18144.594023	29.686183
382.155576	18168.784223	29.691200
382.621324	18198.108954	29.696218
382.875090	18229.527626	29.701236
382.991674	18249.524217	29.706253
383.105266	18276.449721	29.711271
383.586908	18302.138341	29.716288
384.415126	18334.378045	29.721306
384.767264	18356.497070	29.726324
385.170711	18386.480357	29.731341
385.576356	18424.314008	29.736359
385.950275	18439.787995	29.741376
386.409634	18461.561514	29.746394
386.820905	18497.903085	29.751412
387.032027	18507.702068	29.756429
387.489218	18543.624685	29.761447
388.117393	18556.854399	29.766464
388.459912	18584.615870	29.771482
388.468502	18623.069019	29.776500
388.719690	18636.689091	29.781517
388.758044	18677.160038	29.786535
389.260173	18708.886908	29.791552
389.990609	18733.606480	29.796570
389.906933	18765.559678	29.801588
390.458981	18806.784607	29.806605
391.003094	18831.926128	29.811623
391.376780	18865.500116	29.816640
391.935316	18900.096672	29.821658
392.555246	18931.274771	29.826676
392.987668	18958.433955	29.831693
392.664591	18991.040457	29.836711
393.454865	19010.248574	29.841728
393.671912	19039.352669	29.846746
393.880594	19073.146715	29.851764
394.582066	19094.986620	29.856781
394.490877	19122.349386	29.861799
394.839249	19161.868437	29.866816
395.185072	19190.237323	29.871834
395.795079	19230.080563	29.876852
396.545900	19248.395294	29.881869
396.879264	19283.988434	29.886887
397.121162	19305.953544	29.891904
397.512970	19344.355965	29.896922
397.675175	19384.371426	29.901940
398.240265	19407.634271	29.906957
398.503247	19446.212745	29.911975
398.985405	19479.016429	29.916992
399.535094	19516.357329	29.922010
399.957562	19547.287056	29.927028
400.160163	19580.884488	29.932045
400.652730	19612.300924	29.937063
400.665874	19648.329358	29.942080
401.327365	19680.797907	29.947098
401.588044	19726.547599	29.952116
402.264343	19759.745377	29.957133
402.566039	19797.496861	29.962151
403.133762	19836.602826	29.967168
403.429497	19863.902767	29.972186
403.561437	19904.102629	29.977204
404.493639	19941.229821	29.982221
404.909737	19977.997910	29.987239
405.412609	20006.600749	29.992256
406.084501	20033.242764	29.997274
406.203632	20072.089279	30.002292
406.724077	20103.623420	30.007309
407.307414	20122.767742	30.012327
407.146642	20149.809457	30.017344
407.865907	20182.792851	30.022362
408.217506	20229.288790	30.027380
408.598842	20248.619617	30.032397
408.615224	20293.003366	30.037415
409.051933	20323.158049	30.042432
409.561012	20364.419151	30.047450
409.972490	20414.278089	30.052468
410.687281	20441.440247	30.057485
411.238906	20481.021790	30.062503
411.347489	20507.105055	30.067520
411.880501	20545.980344	30.072538
412.002893	20577.016812	30.077556
412.804913	20609.400838	30.082573
413.324569	20652.705808	30.087591
413.464572	20694.279485	30.092608
414.033880	20710.439042	30.097626
414.398984	20756.301963	30.102644
414.804373	20781.221835	30.107661
415.217073	20823.020310	30.112679
415.263340	20851.037952	30.117696
416.090365	20882.300509	30.122714
416.629191	20922.452811	30.127732
417.137876	20961.954297	30.132749
416.996108	20997.407386	30.137767
417.441622	21032.627764	30.142784
417.901164	21063.525767	30.147802
418.251068	21106.555695	30.152820
418.641619	21141.033313	30.157837
419.380649	21183.286373	30.162855
419.465948	21226.767185	30.167872
420.600316	21252.446916	30.172890
420.494219	21298.226889	30.177908
420.865492	21315.597604	30.182925
421.141847	21352.026023	30.187943
421.601973	21387.328290	30.192960
422.329382	21409.188998	30.197978
422.484984	21452.702905	30.202996
423.036678	21485.054361	30.208013
423.462609	21515.145163	30.213031
423.705087	21549.395843	30.218048
424.132934	21576.746075	30.223066
424.498322	21615.506512	30.228084
425.146480	21649.956730	30.233101
425.439172	21676.820203	30.238119
425.564410	21726.407155	30.243136
426.528595	21746.740667	30.248154
426.894105	21794.110561	30.253172
427.438697	21822.550331	30.258189
427.936290	21853.509708	30.263207
428.258445	21872.640908	30.268224
428.536423	21906.790254	30.273242
428.900902	21948.222648	30.278260
429.639550	21984.416672	30.283277
429.979891	22006.192417	30.288295
430.086542	22048.005152	30.293312
430.908171	22080.529098	30.298330
431.424230	22123.305483	30.303348
431.653967	22149.880536	30.308365
432.073244	22196.799581	30.313383
432.498432	22228.692474	30.318400
433.251135	22255.758257	30.323418
433.756352	22295.643445	30.328436
433.791062	22337.348961	30.333453
434.247534	22364.664195	30.338471
434.357399	22409.120019	30.343488
435.582160	22433.793206	30.348506
435.654625	22476.287531	30.353524
436.093227	22502.569973	30.358541
436.233546	22543.541064	30.363559
436.905419	22581.751563	30.368576
437.424725	22615.324701	30.373594
437.586860	22664.301207	30.378612
438.126564	22692.692790	30.383629
438.853534	22735.941984	30.388647
439.118400	22777.845443	30.393664
439.469944	22811.435693	30.398682
439.840918	22846.580725	30.403700
440.341837	22887.737384	30.408717
440.748891	22923.496310	30.413735
441.177926	22965.893429	30.418752
441.399894	23002.504697	30.423770
442.259336	23050.518566	30.428788
442.968814	23084.352883	30.433805
443.556801	23112.946904	30.438823
443.855449	23155.282497	30.443840
444.600219	23182.945560	30.448858
444.679102	23208.055499	30.453876
444.936601	23246.597830	30.458893
445.476909	23276.668102	30.463911
446.101791	23321.591420	30.468928
446.603640	23352.262680	30.473946
447.295962	23385.438138	30.478964
447.404105	23421.017347	30.483981
448.168680	23445.858052	30.488999
448.310941	23481.669855	30.494016
448.887697	23506.221615	30.499034
449.252464	23556.237879	30.504052
449.179248	23577.260925	30.509069
450.057836	23621.572205	30.514087
450.107843	23655.926791	30.519104
450.675688	23676.416527	30.524122
450.781612	23720.633579	30.529140
451.186434	23760.614511	30.534157
451.976679	23790.527638	30.539175
452.105620	23832.465645	30.544192
452.835530	23864.167680	30.549210
452.925881	23900.507767	30.554228
453.516529	23937.910010	30.559245
453.958633	23981.490209	30.564263
454.169144	24027.180973	30.569280
454.954144	24051.481439	30.574298
454.644633	24106.499487	30.579316
455.336295	24149.196714	30.584333
455.920671	24194.677822	30.589351
456.524502	24240.881244	30.594368
456.994689	24290.497429	30.599386
457.411819	24333.104924	30.604404
458.137470	24376.730675	30.609421
458.621722	24409.357492	30.614439
458.811121	24457.487783	30.619456
459.417431	24500.111700	30.624474
459.890676	24544.148665	30.629492
460.178527	24588.512901	30.634509
460.949273	24629.980788	30.639527
461.310620	24672.440657	30.644544
461.706785	24723.823995	30.649562
462.212530	24769.120936	30.654580
462.709069	24808.874665	30.659597
463.403327	24850.888782	30.664615
463.409114	24890.257105	30.669632
464.246617	24931.746216	30.674650
464.904191	24977.261448	30.679668
465.335210	25010.043308	30.684685
465.708452	25054.949743	30.689703
466.120480	25099.092888	30.694720
466.841853	25145.105822	30.699738
467.241838	25183.053307	30.704756
467.575914	25228.026604	30.709773
468.344912	25256.539068	30.714791
468.485145	25311.912362	30.719808
468.975803	25337.118144	30.724826
469.037156	25395.040708	30.729844
469.493034	25439.710527	30.734861
470.319572	25482.363527	30.739879
470.614486	25532.513824	30.744896
471.096031	25576.331270	30.749914
471.835437	25629.571970	30.754932
472.060651	25671.561623	30.759949
472.750632	25714.846563	30.764967
473.198871	25763.596915	30.769984
473.978478	25806.756856	30.775002
474.413928	25844.207869	30.780020
474.537253	25891.971444	30.785037
475.339835	25931.491026	30.790055
475.840382	25985.210796	30.795072
476.243059	26015.598853	30.800090
476.443237	26048.871956	30.805108
477.050541	26101.760615	30.810125
477.676680	26136.180963	30.815143
477.911708	26195.913287	30.820160
478.714219	26230.932350	30.825178
479.078873	26277.874784	30.830196
479.165953	26326.708571	30.835213
479.722626	26364.282599	30.840231
480.429144	26411.645135	30.845248
480.849133	26454.333120	30.850266
481.631613	26493.198055	30.855284
481.625834	26536.032401	30.860301
482.042809	26586.648185	30.865319
482.560694	26627.714812	30.870336
482.995591	26665.082529	30.875354
483.212852	26699.331925	30.880372
483.732804	26748.139433	30.885389
484.538958	26796.700992	30.890407
484.778692	26844.047321	30.895424
485.402435	26874.633738	30.900442
485.780334	26928.698491	30.905460
485.918262	26973.210390	30.910477
486.875081	27023.151390	30.915495
487.287719	27067.734790	30.920512
487.774222	27112.429108	30.925530
488.453548	27162.053661	30.930548
488.440222	27220.319610	30.935565
489.407939	27247.698414	30.940583
489.545144	27291.394229	30.945600
489.895132	27347.332384	30.950618
490.811471	27396.315873	30.955636
491.005890	27447.135034	30.960653
491.903298	27485.658265	30.965671
492.156080	27543.297670	30.970688
492.902624	27593.546405	30.975706
492.895138	27635.614029	30.980724
493.718590	27693.515971	30.985741
494.426575	27739.071160	30.990759
495.252049	27783.373573	30.995776
495.641659	27827.883872	31.000794
496.122596	27863.950008	31.005812
496.625382	27926.047812	31.010829
497.111691	27957.816637	31.015847
497.480952	28000.242370	31.020864
497.890552	28045.317755	31.025882
498.514035	28100.030079	31.030900
498.582194	28149.906857	31.035917
499.452199	28191.657118	31.040935
499.790100	28234.940378	31.045952
500.043157	28285.951031	31.050970
500.701841	28337.207032	31.055988
501.511747	28396.356514	31.061005
501.899338	28441.871918	31.066023
502.434539	28491.804891	31.071040
503.290330	28535.785578	31.076058
503.295097	28581.664395	31.081076
503.865478	28633.279746	31.086093
504.456007	28680.102968	31.091111
504.806164	28735.679602	31.096128
505.594502	28792.060941	31.101146
505.770827	28833.246090	31.106164
506.157012	28883.785325	31.111181
506.965029	28939.927274	31.116199
507.468101	28981.506690	31.121216
507.821508	29036.645223	31.126234
508.597423	29088.537085	31.131252
508.748014	29140.428463	31.136269
509.198902	29194.756340	31.141287
510.225523	29237.924970	31.146304
510.512620	29301.000355	31.151322
511.265152	29345.665853	31.156340
511.330944	29392.587276	31.161357
512.260426	29442.624937	31.166375
512.268519	29508.561416	31.171392
512.829147	29560.780556	31.176410
513.549555	29606.344881	31.181428
513.961745	29669.779488	31.186445
514.483532	29700.939867	31.191463
515.184526	29757.550154	31.196480
515.816200	29817.860266	31.201498
516.297046	29857.836403	31.206516
516.549088	29911.549477	31.211533
517.089273	29945.695029	31.216551
517.653809	29996.015508	31.221568
518.055765	30042.845185	31.226586
518.815067	30081.624176	31.231604
518.753316	30139.582900	31.236621
519.272202	30184.752988	31.241639
519.665014	30231.218696	31.246656
520.132150	30297.580678	31.251674
521.009685	30345.525085	31.256692
521.069557	30395.990161	31.261709
521.761960	30450.638489	31.266727
522.271207	30514.583831	31.271744
522.846501	30566.055776	31.276762
523.746414	30624.235587	31.281780
523.966363	30685.512857	31.286797
524.567593	30733.661799	31.291815
524.807112	30794.702730	31.296832
525.318515	30850.603294	31.301850
526.140155	30908.793842	31.306868
526.487795	30975.294891	31.311885
526.978877	31028.425973	31.316903
527.717696	31076.565707	31.321920
528.243985	31131.985109	31.326938
528.843774	31185.540407	31.331956
529.197192	31252.887146	31.336973
529.801923	31320.539636	31.341991
530.387885	31375.233687	31.347008
531.093144	31434.123606	31.352026
531.659804	31496.968132	31.357044
532.208582	31555.900125	31.362061
532.454552	31608.464537	31.367079
532.843766	31668.265771	31.372096
533.489086	31736.146628	31.377114
534.369601	31784.324799	31.382132
534.807683	31844.424609	31.387149
535.704526	31897.289224	31.392167
536.261955	31950.169137	31.397184
536.864178	32005.837454	31.402202
537.682286	32045.974162	31.407220
537.952778	32108.876176	31.412237
538.690671	32149.704800	31.417255
539.091048	32201.570169	31.422272
539.645848	32251.258147	31.427290
540.331075	32287.649827	31.432308
540.964093	32349.277873	31.437325
541.358294	32397.560268	31.442343
541.782441	32438.520356	31.447360
542.029931	32498.877957	31.452378
542.847729	32548.314992	31.457396
543.080917	32612.121113	31.462413
543.791105	32655.318939	31.467431
544.835995	32720.385871	31.472448
544.757581	32776.888679	31.477466
545.867211	32822.368518	31.482484
546.129205	32883.782123	31.487501
546.569927	32929.382380	31.492519
547.018097	32980.166077	31.497536
547.444594	33048.441583	31.502554
548.037239	33098.706292	31.507572
548.574454	33155.903642	31.512589
548.911554	33207.921263	31.517607
549.789818	33264.437727	31.522624
550.210347	33334.255245	31.527642
551.121982	33381.627929	31.532660
551.298591	33435.578759	31.537677
551.870400	33489.776771	31.542695
552.303441	33538.567047	31.547712
553.090467	33588.507502	31.552730
553.701863	33638.852680	31.557748
554.109603	33691.772009	31.562765
554.641016	33741.644738	31.567783
555.050323	33788.356878	31.572800
555.542330	33859.411118	31.577818
556.126855	33900.442706	31.582836
556.895222	33957.260408	31.587853
557.010197	34016.035655	31.592871
557.609816	34070.817794	31.597888
558.079437	34134.874258	31.602906
558.611057	34191.009208	31.607924
558.984883	34250.569204	31.612941
559.534140	34317.077797	31.617959
560.316930	34373.651442	31.622976
560.359005	34436.886636	31.627994
561.363720	34501.439699	31.633012
562.125940	34567.131344	31.638029
562.534295	34638.180425	31.643047
562.948499	34700.048460	31.648064
563.537973	34766.400585	31.653082
564.050322	34821.385655	31.658100
564.873423	34901.336133	31.663117
565.291415	34959.714032	31.668135
566.305799	35018.779265	31.673152
566.576848	35091.951533	31.678170
567.077347	35147.479223	31.683188
567.591961	35220.794760	31.688205
568.240819	35279.700414	31.693223
569.101139	35343.743889	31.698240
569.460477	35411.225278	31.703258
570.172870	35468.372629	31.708276
570.874331	35535.690576	31.713293
571.085136	35601.025929	31.718311
572.250741	35655.671923	31.723328
572.527602	35722.934581	31.728346
573.070272	35789.266664	31.733364
573.556264	35861.690074	31.738381
574.052585	35923.902209	31.743399
574.946709	35983.785837	31.748416
575.412170	36051.031137	31.753434
576.025951	36107.010143	31.758452
576.510359	36177.370998	31.763469
577.118819	36237.261702	31.768487
577.820317	36304.573045	31.773504
578.065452	36369.236397	31.778522
578.819438	36441.772444	31.783540
579.405288	36501.557300	31.788557
579.556646	36578.473356	31.793575
580.595956	36642.605453	31.798592
581.081257	36707.318650	31.803610
581.839072	36772.798136	31.808628
582.391651	36834.240293	31.813645
582.823731	36901.888805	31.818663
583.744987	36961.515532	31.823680
584.217815	37037.786975	31.828698
584.593242	37104.454552	31.833716
585.198464	37165.942780	31.838733
585.816341	37235.922693	31.843751
586.820551	37298.292243	31.848768
586.902436	37365.192410	31.853786
587.743206	37429.432738	31.858804
588.426492	37502.025759	31.863821
588.576597	37559.749359	31.868839
589.463623	37620.760083	31.873856
589.589152	37694.453030	31.878874
590.112250	37767.187241	31.883892
591.246663	37830.130477	31.888909
591.675439	37895.788396	31.893927
592.217676	37956.803634	31.898944
592.546274	38015.458697	31.903962
593.692593	38068.224480	31.908980
594.362010	38130.049399	31.913997
594.617917	38183.392108	31.919015
595.570184	38243.472444	31.924032
595.760746	38307.394170	31.929050
596.068341	38370.059414	31.934068
596.659220	38431.759464	31.939085
597.263413	38508.952817	31.944103
597.851067	38573.147521	31.949120
598.374925	38639.815100	31.954138
599.146383	38707.941315	31.959156
599.542204	38782.146328	31.964173
599.912768	38852.564781	31.969191
600.838295	38922.345601	31.974208
601.585458	39005.710609	31.979226
601.949431	39080.525009	31.984244
602.888218	39139.508869	31.989261
603.123981	39226.914735	31.994279
604.025768	39293.193878	31.999296
604.604856	39365.609526	32.004314
605.449085	39433.391798	32.009332
606.148383	39505.674471	32.014349
606.340827	39581.639916	32.019367
607.070085	39652.674474	32.024384
607.579278	39733.294791	32.029402
608.002365	39803.326241	32.034420
608.818713	39869.880457	32.039437
609.616388	39940.904811	32.044455
609.929327	40010.551210	32.049472
610.464846	40094.319207	32.054490
610.871304	40167.170644	32.059508
611.827986	40243.422765	32.064525
612.408616	40328.582831	32.069543
613.178899	40404.512895	32.074560
613.882569	40483.339652	32.079578
614.109682	40564.849999	32.084596
615.317926	40636.143739	32.089613
615.795911	40707.956337	32.094631
616.483696	40780.321689	32.099648
616.757735	40863.830224	32.104666
617.554762	40930.940774	32.109684
618.383112	41004.496008	32.114701
618.713379	41076.706998	32.119719
619.366120	41151.169501	32.124736
620.353883	41242.627707	32.129754
620.394811	41304.128475	32.134772
621.158998	41382.159809	32.139789
621.534957	41468.318718	32.144807
622.489506	41539.907325	32.149824
623.263559	41620.599407	32.154842
624.177195	41701.732835	32.159860
624.722657	41770.835956	32.164877
625.248269	41845.865301	32.169895
626.065597	41914.112609	32.174912
626.747672	41979.847390	32.179930
627.229902	42050.881534	32.184948
627.926407	42118.751788	32.189965
628.485345	42195.608166	32.194983
629.253711	42265.449750	32.200000
629.635388	42334.181106	32.205018
630.006210	42413.601552	32.210036
630.988204	42481.435371	32.215053
631.349177	42568.425888	32.220071
632.337907	42634.863668	32.225088
632.899699	42701.981662	32.230106
633.271087	42773.999859	32.235124
633.836015	42830.294789	32.240141
634.808582	42904.449362	32.245159
635.405408	42963.767231	32.250176
635.852548	43029.787700	32.255194
636.178406	43104.422619	32.260212
637.179078	43163.049166	32.265229
637.521778	43252.638043	32.270247
638.103129	43319.262481	32.275264
638.830052	43390.387544	32.280282
639.503281	43466.731395	32.285300
639.976357	43536.023540	32.290317
640.198313	43624.936397	32.295335
641.278212	43696.967233	32.300352
641.778746	43776.491997	32.305370
642.504586	43858.881495	32.310388
643.198868	43934.226026	32.315405
643.855304	44011.089538	32.320423
644.644381	44078.942137	32.325440
645.261678	44160.248964	32.330458
645.908570	44235.750948	32.335476
646.778234	44318.608083	32.340493
647.461241	44404.344540	32.345511
647.980186	44470.563448	32.350528
648.267865	44549.498356	32.355546
648.743472	44632.273661	32.360564
649.600327	44713.287489	32.365581
650.758578	44796.597886	32.370599
651.207539	44870.647947	32.375616
651.820441	44955.937508	32.380634
652.333311	45034.262509	32.385652
653.297321	45113.400496	32.390669
654.067358	45192.419340	32.395687
654.324046	45271.457128	32.400704
655.409574	45348.545627	32.405722
656.042678	45432.207800	32.410740
657.060511	45501.180245	32.415757
657.574904	45583.624911	32.420775
658.412225	45652.716188	32.425792
659.111724	45733.223622	32.430810
659.609933	45807.723927	32.435828
660.447204	45877.548632	32.440845
660.854372	45959.933734	32.445863
661.378994	46035.538944	32.450880
662.103209	46106.134749	32.455898
662.455739	46185.722590	32.460916
663.465166	46268.776751	32.465933
664.191273	46344.040394	32.470951
664.737941	46421.456096	32.475968
665.356945	46505.103242	32.480986
665.957906	46582.974827	32.486004
666.649655	46657.200140	32.491021
666.962499	46744.941087	32.496039
667.545108	46821.351418	32.501056
668.104970	46910.792279	32.506074
669.051338	46994.573742	32.511092
670.009398	47071.848248	32.516109
670.660108	47162.364758	32.521127
671.278957	47238.925512	32.526144
671.842104	47316.850570	32.531162
672.526453	47404.248880	32.536180
673.659629	47476.534823	32.541197
673.944462	47564.502084	32.546215
674.638062	47644.617529	32.551232
675.556196	47731.561802	32.556250
676.051201	47819.640741	32.561268
676.666079	47883.531365	32.566285
677.445078	47971.390329	32.571303
678.245321	48046.585281	32.576320
678.799051	48112.419556	32.581338
678.980673	48182.708587	32.586356
679.824133	48248.435396	32.591373
680.595258	48330.009432	32.596391
681.347032	48413.068202	32.601408
681.881925	48485.381143	32.606426
682.363287	48576.725078	32.611444
683.167801	48651.249002	32.616461
683.406548	48739.153488	32.621479
684.146607	48814.383521	32.626496
684.790160	48897.759168	32.631514
685.612995	48996.704234	32.636532
686.132667	49080.903371	32.641549
686.312289	49185.438601	32.646567
687.350080	49270.396127	32.651584
688.202948	49361.300179	32.656602
688.654642	49463.865329	32.661620
689.633366	49548.578028	32.666637
690.316423	49638.538704	32.671655
690.802879	49730.206272	32.676672
691.762288	49828.365531	32.681690
692.193210	49925.298809	32.686708
693.222060	50013.302658	32.691725
693.769774	50114.579374	32.696743
694.484172	50211.325063	32.701760
695.430587	50290.484297	32.706778
695.909539	50388.747994	32.711796
696.946390	50473.148765	32.716813
697.737306	50570.793248	32.721831
698.152076	50674.305859	32.726848
699.172586	50762.526124	32.731866
699.753755	50852.670394	32.736884
700.466326	50938.788251	32.741901
701.351298	51032.528118	32.746919
701.934212	51129.483344	32.751936
703.014835	51211.953336	32.756954
703.396201	51297.931739	32.761972
704.419713	51386.457578	32.766989
704.783137	51482.345341	32.772007
705.796091	51567.039111	32.777024
706.696036	51650.621127	32.782042
707.276778	51741.938317	32.787060
707.994684	51824.186623	32.792077
708.745552	51915.388040	32.797095
709.158558	52001.459079	32.802112
709.939521	52087.558078	32.807130
710.674686	52189.604305	32.812148
711.865787	52272.325858	32.817165
712.334186	52354.017500	32.822183
712.944087	52440.234798	32.827200
713.875205	52523.379483	32.832218
714.177929	52624.697169	32.837236
715.018958	52706.884606	32.842253
715.591385	52796.287506	32.847271
716.167826	52893.694822	32.852288
716.986031	52977.833061	32.857306
717.703055	53071.250399	32.862324
718.467518	53162.891323	32.867341
719.167169	53250.954810	32.872359
719.676075	53348.445055	32.877376
720.448707	53437.167010	32.882394
720.855470	53540.430795	32.887412
721.732092	53631.480413	32.892429
722.569706	53730.428194	32.897447
723.027001	53826.596231	32.902464
723.871225	53920.179793	32.907482
724.418750	54024.800192	32.912500
725.437127	54114.438598	32.917517
726.122609	54198.572430	32.922535
726.670873	54287.202651	32.927552
727.704836	54375.493877	32.932570
728.383840	54465.297428	32.937588
728.743694	54549.726719	32.942605
729.767814	54642.228788	32.947623
730.312359	54739.555744	32.952640
730.960569	54815.377029	32.957658
731.713129	54927.556736	32.962676
732.504474	55020.509782	32.967693
733.275487	55115.785527	32.972711
734.219996	55208.278140	32.977728
735.187611	55292.660618	32.982746
735.525378	55392.653520	32.987764
736.172892	55484.128702	32.992781
737.195918	55583.326801	32.997799
737.583913	55682.131260	33.002816
738.543785	55777.638014	33.007834
738.912654	55870.854491	33.012852
739.970532	55974.415049	33.017869
740.812630	56070.884195	33.022887
741.197888	56166.487865	33.027904
742.281892	56266.980977	33.032922
743.041826	56373.998784	33.037940
743.851704	56469.533671	33.042957
744.612592	56568.394589	33.047975
744.909797	56672.419508	33.052992
746.076094	56768.794175	33.058010
746.648587	56874.929411	33.063028
747.221590	56980.294192	33.068045
747.892759	57080.183544	33.073063
748.824024	57186.159980	33.078080
750.052959	57285.155559	33.083098
750.502323	57398.915960	33.088116
751.348423	57495.814721	33.093133
751.926132	57599.039744	33.098151
752.447246	57695.658302	33.103168
753.568335	57801.391738	33.108186
753.915577	57913.832241	33.113204
754.889409	58019.717572	33.118221
755.880292	58123.148683	33.123239
756.603423	58227.768447	33.128256
757.459720	58322.874772	33.133274
758.599471	58432.084189	33.138292
759.069659	58531.464204	33.143309
759.969810	58618.254388	33.148327
760.719706	58724.452214	33.153344
761.778902	58816.000933	33.158362
762.124764	58916.477758	33.163380
762.867871	59027.373860	33.168397
764.170972	59121.582161	33.173415
764.383170	59223.365538	33.178432
765.170732	59324.232676	33.183450
765.625786	59426.406654	33.188468
766.636857	59521.929103	33.193485
767.832353	59633.866009	33.198503
768.231251	59745.417055	33.203520
769.246656	59838.399646	33.208538
769.987333	59940.225610	33.213556
770.200284	60040.243348	33.218573
771.203101	60137.912573	33.223591
772.201440	60250.700788	33.228608
772.942130	60353.009150	33.233626
773.476071	60462.968075	33.238644
774.507540	60566.885312	33.243661
775.442522	60662.836533	33.248679
775.815409	60766.604589	33.253696
776.858375	60860.010757	33.258714
777.384111	60948.642547	33.263732
777.842373	61048.896438	33.268749
778.574600	61146.621581	33.273767
779.355782	61251.506487	33.278784
780.139385	61349.527485	33.283802
780.781409	61460.023787	33.288820
781.462239	61557.196868	33.293837
782.524634	61660.608916	33.298855
782.937391	61774.279844	33.303872
783.882759	61887.395579	33.308890
784.784056	61996.208521	33.313908
785.401571	62104.007098	33.318925
786.254170	62208.328870	33.323943
786.893259	62328.437879	33.328960
788.077443	62416.929191	33.333978
788.583555	62533.275225	33.338996
789.451367	62652.520265	33.344013
790.433557	62764.983692	33.349031
791.116896	62881.637389	33.354048
791.873455	62987.906892	33.359066
792.681009	63096.810694	33.364084
793.477555	63205.268097	33.369101
794.362950	63328.976807	33.374119
794.958317	63448.619173	33.379136
796.012801	63556.795556	33.384154
796.725956	63665.781184	33.389172
797.358456	63782.334594	33.394189
798.617990	63893.841721	33.399207
799.057096	64014.739529	33.404224
799.940186	64129.982866	33.409242
800.661920	64242.010668	33.414260
801.558131	64358.523700	33.419277
802.748810	64465.847880	33.424295
803.669115	64586.384962	33.429312
804.604793	64698.209160	33.434330
805.353742	64806.025377	33.439348
806.008462	64913.788200	33.444365
807.121553	65017.828200	33.449383
807.966337	65133.538593	33.454400
808.562852	65244.802300	33.459418
809.428384	65344.301662	33.464436
809.949904	65461.116740	33.469453
810.933366	65572.337159	33.474471
811.657263	65689.657393	33.479488
812.476365	65807.809665	33.484506
813.333968	65916.473418	33.489524
814.474560	66028.567982	33.494541
814.998446	66133.020763	33.499559
815.747721	66252.912986	33.504576
816.679487	66356.047665	33.509594
817.653351	66474.671218	33.514612
818.267132	66584.655813	33.519629
818.955042	66691.221106	33.524647
819.679617	66818.783043	33.529664
820.460449	66931.574146	33.534682
821.386103	67040.649727	33.539700
822.261158	67172.273069	33.544717
823.210164	67277.211258	33.549735
823.922418	67394.808477	33.554752
825.096309	67498.528299	33.559770
825.857795	67618.894136	33.564788
826.449216	67739.750323	33.569805
827.439612	67843.192389	33.574823
828.229002	67963.416478	33.579840
828.992688	68075.350346	33.584858
829.819808	68175.255136	33.589876
830.538535	68288.537948	33.594893
831.388453	68390.267208	33.599911
832.335791	68508.710579	33.604928
832.996313	68612.350056	33.609946
833.863281	68719.496616	33.614964
834.674168	68821.936221	33.619981
835.380528	68918.760014	33.624999
836.579052	69043.746835	33.630016
837.284167	69135.425050	33.635034
838.133487	69254.773987	33.640052
838.619441	69367.822840	33.645069
839.534915	69482.242886	33.650087
840.156673	69582.365293	33.655104
840.828578	69698.281064	33.660122
841.713719	69819.922487	33.665140
842.149686	69940.500735	33.670157
843.494346	70059.727986	33.675175
844.287643	70192.743032	33.680192
845.321864	70319.971279	33.685210
846.147029	70423.295130	33.690228
846.589725	70558.204161	33.695245
847.609788	70681.282511	33.700263
848.485933	70806.845143	33.705280
849.180988	70939.318287	33.710298
850.360100	71054.322817	33.715316
850.697284	71174.058022	33.720333
852.075920	71302.784370	33.725351
852.913972	71433.409418	33.730368
853.816358	71555.620613	33.735386
854.967019	71681.111324	33.740404
855.632773	71808.693873	33.745421
856.814424	71927.136370	33.750439
857.559750	72053.657477	33.755456
858.406263	72173.111625	33.760474
859.605080	72294.569716	33.765492
860.205900	72420.459192	33.770509
861.137020	72531.876418	33.775527
861.794136	72657.214107	33.780544
862.900050	72776.913255	33.785562
863.848314	72898.903107	33.790580
864.528111	73027.375856	33.795597
865.576251	73153.429587	33.800615
866.639394	73271.019983	33.805632
867.318061	73394.176555	33.810650
868.350227	73511.305389	33.815668
868.927593	73641.550479	33.820685
869.675099	73759.258950	33.825703
870.829519	73887.727840	33.830720
871.354285	74020.475633	33.835738
872.499206	74132.441196	33.840756
873.346880	74268.368809	33.845773
874.273698	74392.356399	33.850791
874.821993	74516.546428	33.855808
875.696041	74643.288958	33.860826
876.977457	74767.479328	33.865844
877.748851	74888.782223	33.870861
878.256188	75015.138504	33.875879
879.484033	75144.595570	33.880896
880.372423	75275.121478	33.885914
881.320885	75396.499082	33.890932
882.004070	75515.479892	33.895949
883.257988	75644.246191	33.900967
883.931207	75766.645360	33.905984
884.943353	75896.819267	33.911002
885.968737	76015.916950	33.916020
886.595132	76145.839875	33.921037
887.696934	76260.511472	33.926055
888.578640	76373.044282	33.931072
889.412393	76500.727590	33.936090
890.225964	76599.718390	33.941108
891.075623	76725.104381	33.946125
891.997113	76840.030171	33.951143
892.805464	76955.924033	33.956160
893.576370	77068.320563	33.961178
894.651884	77180.123321	33.966196
895.261774	77303.389015	33.971213
896.040502	77419.334465	33.976231
896.861275	77540.472940	33.981248
897.710639	77678.540203	33.986266
898.958493	77796.105214	33.991284
899.705938	77922.628109	33.996301
900.429521	78039.490428	34.001319
901.629982	78150.790331	34.006336
902.410639	78287.095264	34.011354
903.009878	78413.892138	34.016372
903.814946	78546.709249	34.021389
905.069465	78673.076620	34.026407
905.985596	78811.475083	34.031424
906.626645	78940.798271	34.036442
907.849095	79067.242745	34.041460
908.748658	79195.841472	34.046477
909.865194	79319.357082	34.051495
910.834037	79449.394403	34.056512
911.603602	79587.998999	34.061530
913.075721	79703.784657	34.066548
913.781571	79827.586047	34.071565
914.813979	79952.523390	34.076583
915.812159	80083.824703	34.081600
916.599240	80210.031280	34.086618
917.530695	80323.075461	34.091636
918.545122	80452.541669	34.096653
919.301456	80575.364579	34.101671
920.609119	80711.457837	34.106688
921.188348	80834.558156	34.111706
922.395791	80952.032454	34.116724
923.214729	81095.882554	34.121741
923.787852	81212.387626	34.126759
924.926181	81339.105431	34.131776
925.476223	81481.939609	34.136794
926.766145	81602.851502	34.141812
927.443393	81741.085942	34.146829
927.967648	81872.849216	34.151847
929.335051	82018.215031	34.156864
930.234497	82144.945178	34.161882
931.397037	82281.204662	34.166900
932.027846	82414.357934	34.171917
932.856375	82547.605816	34.176935
933.690695	82679.777973	34.181952
934.615877	82822.520512	34.186970
935.929688	82963.763491	34.191988
936.622931	83103.148641	34.197005
937.802182	83245.896080	34.202023
938.806571	83375.234980	34.207040
939.575578	83519.880428	34.212058
940.721881	83642.231398	34.217076
941.356291	83786.818524	34.222093
942.284466	83914.521696	34.227111
943.734566	84049.851981	34.232128
944.487181	84193.890627	34.237146
945.568860	84325.107543	34.242164
946.955053	84462.918401	34.247181
947.451711	84591.253452	34.252199
948.548955	84717.028591	34.257216
949.566982	84851.776969	34.262234
950.729649	84971.405183	34.267252
951.647358	85108.322929	34.272269
952.532673	85222.531448	34.277287
953.764039	85339.714144	34.282304
954.334310	85459.765524	34.287322
955.139656	85576.722466	34.292340
956.032782	85689.223552	34.297357
956.790769	85818.971150	34.302375
957.537341	85940.856150	34.307392
958.671694	86071.099738	34.312410
959.778190	86201.892837	34.317428
960.536897	86333.142820	34.322445
961.221695	86449.282468	34.327463
962.317952	86578.307592	34.332480
963.300262	86720.995015	34.337498
964.129788	86840.498041	34.342516
965.084177	86984.957149	34.347533
966.048378	87119.847710	34.352551
966.781214	87248.272170	34.357568
967.912066	87393.223490	34.362586
968.834807	87535.501718	34.367604
970.070253	87675.634505	34.372621
970.954899	87817.148702	34.377639
972.092761	87942.871143	34.382656
972.863229	88089.898671	34.387674
973.502140	88233.094981	34.392692
974.922454	88370.486507	34.397709
976.100015	88516.569735	34.402727
977.177328	88651.621183	34.407744
978.147532	88799.335173	34.412762
979.032745	88934.774380	34.417780
980.320402	89077.115418	34.422797
980.814962	89217.145656	34.427815
982.145199	89349.577221	34.432832
982.951519	89498.309883	34.437850
984.133201	89624.540246	34.442868
985.371973	89771.924729	34.447885
986.162426	89912.745488	34.452903
987.217808	90048.833706	34.457920
988.070073	90196.044215	34.462938
989.282813	90324.329966	34.467956
990.292772	90467.396037	34.472973
991.079836	90613.392095	34.477991
992.491737	90750.311372	34.483008
993.125294	90903.758344	34.488026
994.199882	91036.792109	34.493044
995.106998	91177.904769	34.498061
995.971484	91327.430250	34.503079
997.031735	91473.398996	34.508096
998.277702	91611.407547	34.513114
999.253432	91765.467964	34.518132
1000.203605	91901.109343	34.523149
1001.270657	92037.061273	34.528167
1002.633746	92182.832315	34.533184
1003.398643	92322.835892	34.538202
1004.358466	92467.384144	34.543220
1005.773558	92605.826095	34.548237
1006.527956	92737.795507	34.553255
1007.623826	92885.944160	34.558272
1008.474324	93026.152822	34.563290
1009.517253	93164.513903	34.568308
1010.575939	93298.410835	34.573325
1011.467961	93446.995355	34.578343
1012.349602	93581.897866	34.583360
1013.597024	93736.090378	34.588378
1014.439766	93879.925771	34.593396
1015.384237	94016.257120	34.598413
1016.599955	94157.918342	34.603431
1017.440800	94295.515335	34.608448
1018.209823	94443.898348	34.613466
1019.475022	94583.895422	34.618484
1020.495588	94711.603086	34.623501
1021.322034	94850.528507	34.628519
1022.645399	94982.764053	34.633536
1023.686510	95115.933177	34.638554
1024.358269	95254.601592	34.643572
1025.315858	95377.727499	34.648589
1026.340373	95515.706042	34.653607
1027.482797	95646.531786	34.658624
1028.169733	95781.795022	34.663642
1029.087474	95931.339771	34.668660
1030.307757	96070.580390	34.673677
1030.840722	96218.437004	34.678695
1031.896902	96367.904512	34.683712
1033.006762	96520.554543	34.688730
1033.819186	96669.608374	34.693748
1035.028476	96830.454390	34.698765
1035.906059	96984.626982	34.703783
1036.923431	97138.910351	34.708800
1037.915712	97297.066790	34.713818
1039.211331	97460.257543	34.718836
1040.424805	97615.391371	34.723853
1041.378111	97781.483266	34.728871
1042.607556	97928.722027	34.733888
1043.536309	98089.381925	34.738906
1044.769005	98244.389835	34.743924
1045.711018	98411.038523	34.748941
1046.703170	98573.007829	34.753959
1048.036288	98725.279808	34.758976
1048.791511	98887.201664	34.763994
1050.046427	99037.956361	34.769012
1051.387998	99194.224619	34.774029
1051.630600	99365.274998	34.779047
1052.684650	99530.785588	34.784064
1054.283443	99697.960919	34.789082
1055.155833	99865.630990	34.794100
1056.331432	100024.464268	34.799117
1057.251215	100190.267250	34.804135
1058.520388	100345.668161	34.809152
1059.530904	100511.059348	34.814170
1060.444917	100672.244513	34.819188
1062.001008	100841.295818	34.824205
1062.817099	101020.645282	34.829223
1064.200619	101172.144765	34.834240
1065.400795	101340.118524	34.839258
1066.319362	101498.389266	34.844276
1067.380851	101650.862893	34.849293
1068.267365	101822.753956	34.854311
1069.434208	101971.273749	34.859328
1070.374024	102133.635163	34.864346
1071.544062	102306.609619	34.869364
1073.051728	102465.162460	34.874381
1073.908430	102623.975860	34.879399
1074.843330	102793.427591	34.884416
1076.105819	102950.200337	34.889434
1076.636608	103126.565896	34.894452
1078.067531	103292.405610	34.899469
1078.598697	103448.403114	34.904487
1080.136777	103618.722962	34.909504
1081.157831	103785.456749	34.914522
1081.910149	103966.242859	34.919540
1083.413560	104129.555684	34.924557
1084.438072	104301.028698	34.929575
1085.767103	104466.094831	34.934592
1086.854519	104631.949167	34.939610
1087.774001	104790.081449	34.944628
1089.166851	104961.155921	34.949645
1090.148363	105123.092078	34.954663
1090.968882	105273.442003	34.959680
1092.190987	105435.948223	34.964698
1093.286045	105592.460481	34.969716
1094.473840	105745.462719	34.974733
1095.260401	105897.012335	34.979751
1096.302313	106053.156139	34.984768
1097.125668	106212.174062	34.989786
1098.013839	106377.742981	34.994804
1099.388462	106525.487949	34.999821
1100.426540	106697.670866	35.004839
1101.752014	106862.245902	35.009856
1102.869730	107020.308045	35.014874
1103.502989	107187.076723	35.019892
1104.749318	107352.098502	35.024909
1105.968258	107523.180223	35.029927
1106.949082	107686.892683	35.034944
1108.022434	107853.757410	35.039962
1109.232468	108039.498761	35.044980
1110.368944	108206.519903	35.049997
1111.197049	108385.094249	35.055015
1112.284184	108565.856275	35.060032
1113.497795	108743.824597	35.065050
1114.346321	108921.968448	35.070068
1115.841355	109103.515305	35.075085
1116.764790	109282.649824	35.080103
1118.267848	109458.573615	35.085120
1119.312675	109643.276596	35.090138
1120.125507	109824.776385	35.095156
1121.398389	109996.865553	35.100173
1122.533130	110183.824773	35.105191
1123.712150	110370.131913	35.110208
1124.566116	110554.644602	35.115226
1126.321933	110737.590669	35.120244
1127.726161	110917.720517	35.125261
1128.864410	111095.589985	35.130279
1130.027141	111280.981262	35.135296
1131.411946	111459.306368	35.140314
1132.121367	111638.352347	35.145332
1133.788795	111806.536569	35.150349
1134.835283	111992.661262	35.155367
1136.030701	112165.663602	35.160384
1137.122799	112332.767989	35.165402
1137.481864	112520.428724	35.170420
1139.407269	112688.372964	35.175437
1140.289868	112875.214774	35.180455
1141.176074	113053.632578	35.185472
1142.599677	113234.623121	35.190490
1143.275679	113413.926786	35.195508
1144.316778	113600.620565	35.200525
1145.726375	113792.448962	35.205543
1146.946092	113975.543056	35.210560
1148.202718	114175.418894	35.215578
1149.388917	114357.178088	35.220596
1150.590541	114528.255659	35.225613
1151.637237	114724.521337	35.230631
1152.957014	114912.698102	35.235648
1153.979715	115097.846522	35.240666
1154.940576	115275.848015	35.245684
1155.909001	115472.486580	35.250701
1157.095379	115663.857834	35.255719
1158.304534	115853.148746	35.260736
1159.580601	116033.586194	35.265754
1160.768196	116230.219114	35.270772
1161.808236	116408.277967	35.275789
1162.875267	116615.981869	35.280807
1164.183928	116802.538533	35.285824
1165.581215	116989.474548	35.290842
1166.602845	117181.998225	35.295860
1167.702856	117368.111586	35.300877
1168.971519	117545.126069	35.305895
1169.884954	117722.998622	35.310912
1170.626936	117898.024337	35.315930
1171.849034	118082.158156	35.320948
1172.765854	118254.128781	35.325965
1173.766719	118450.186902	35.330983
1175.281560	118647.643912	35.336000
1176.526541	118833.273926	35.341018
1177.570953	119027.187311	35.346036
1178.798596	119224.353596	35.351053
1180.097184	119408.571896	35.356071
1181.011589	119591.663741	35.361088
1182.297466	119784.819975	35.366106
1183.210229	120005.169360	35.371124
1184.408839	120195.998462	35.376141
1185.793849	120395.566957	35.381159
1186.655694	120599.367035	35.386176
1187.996452	120798.603439	35.391194
1189.395647	121011.479466	35.396212
1190.828004	121212.731078	35.401229
1191.805881	121412.031612	35.406247
1192.670351	121617.206901	35.411264
1194.130868	121829.609804	35.416282
1195.234347	122037.029544	35.421300
1196.415574	122244.957461	35.426317
1197.736540	122452.407510	35.431335
1198.888870	122668.517114	35.436352
1200.189118	122874.085261	35.441370
1201.415763	123082.683176	35.446388
1202.847199	123293.213030	35.451405
1203.796837	123514.076657	35.456423
1205.181888	123729.027524	35.461440
1206.651098	123926.603429	35.466458
1208.039093	124142.190430	35.471476
1209.405623	124351.635825	35.476493
1210.768472	124553.352334	35.481511
1211.815557	124755.553290	35.486528
1213.356007	124957.978215	35.491546
1214.389542	125165.887377	35.496564
1215.658631	125361.325810	35.501581
1216.758951	125578.275997	35.506599
1217.989193	125780.352096	35.511616
1219.337950	125987.809182	35.516634
1220.212843	126190.453698	35.521652
1221.367828	126406.906425	35.526669
1222.408368	126614.406023	35.531687
1223.668432	126834.139769	35.536704
1225.215438	127038.377177	35.541722
1226.100327	127258.442129	35.546740
1227.586545	127466.203335	35.551757
1228.905831	127682.244934	35.556775
1230.253649	127898.904401	35.561792
1231.572439	128106.342670	35.566810
1232.665206	128324.809107	35.571828
1233.522084	128541.871080	35.576845
1234.886167	128746.314745	35.581863
1236.065398	128975.900454	35.586880
1237.235865	129180.087420	35.591898
1238.593149	129399.861256	35.596916
1239.653234	129621.929362	35.601933
1241.065201	129835.308620	35.606951
1242.013409	130068.286915	35.611968
1243.461301	130280.573114	35.616986
1244.620095	130510.566346	35.622004
1245.794850	130727.147184	35.627021
1247.165042	130942.898589	35.632039
1248.522837	131164.687460	35.637056
1249.675326	131380.211608	35.642074
1250.724845	131591.761119	35.647092
1252.195705	131799.807021	35.652109
1253.244460	131995.361427	35.657127
1254.456403	132217.764840	35.662144
1255.908372	132417.476542	35.667162
1256.870364	132629.402314	35.672180
1257.931582	132842.175116	35.677197
1259.691777	133052.957573	35.682215
1260.572419	133277.945804	35.687232
1261.614237	133481.535042	35.692250
1262.968906	133705.535122	35.697268
1264.047863	133925.221270	35.702285
1265.645597	134140.031041	35.707303
1266.597105	134369.147983	35.712320
1268.064655	134590.637992	35.717338
1269.225684	134823.729644	35.722356
1270.410592	135042.176035	35.727373
1271.921982	135263.460494	35.732391
1273.053622	135498.171886	35.737408
1274.628119	135729.870418	35.742426
1275.870865	135961.840937	35.747444
1277.179624	136182.936840	35.752461
1278.456497	136411.088684	35.757479
1279.346104	136655.597983	35.762496
1280.581319	136889.084962	35.767514
1282.008649	137124.430945	35.772532
1283.121954	137365.688083	35.777549
1284.503579	137612.265770	35.782567
1285.764684	137846.021398	35.787584
1287.210665	138090.525286	35.792602
1288.533561	138343.356130	35.797620
1289.643570	138578.282931	35.802637
1291.546486	138816.947503	35.807655
1292.684972	139065.376455	35.812672
1294.009492	139306.105372	35.817690
1295.246783	139544.187693	35.822708
1296.829008	139781.403164	35.827725
1298.082988	140022.744739	35.832743
1299.152259	140264.980772	35.837760
1300.538790	140503.958049	35.842778
1301.835589	140748.252072	35.847796
1303.362197	140994.754227	35.852813
1305.075391	141232.592074	35.857831
1306.082539	141470.332682	35.862848
1307.215103	141707.914706	35.867866
1308.420281	141953.868147	35.872884
1309.549466	142199.087729	35.877901
1311.324012	142440.854679	35.882919
1312.158045	142696.727561	35.887936
1313.717337	142938.368671	35.892954
1314.952428	143183.336702	35.897972
1316.126714	143437.484859	35.902989
1317.959596	143683.587625	35.908007
1318.784471	143933.561609	35.913024
1320.111786	144182.870975	35.918042
1321.577788	144430.092106	35.923060
1322.598286	144685.859798	35.928077
1324.016149	144929.592266	35.933095
1325.303371	145190.569648	35.938112
1326.539159	145444.595160	35.943130
1328.305706	145710.278115	35.948148
1329.339089	145971.176299	35.953165
1330.675036	146221.614438	35.958183
1331.975432	146475.091206	35.963200
1333.424121	146718.285356	35.968218
1335.096168	146975.622989	35.973236
1336.462015	147235.701705	35.978253
1337.682501	147470.086307	35.983271
1338.976726	147709.393723	35.988288
1340.056880	147939.391004	35.993306
1341.273051	148178.270485	35.998324
1342.148209	148436.942258	36.003341
1343.864411	148669.946261	36.008359
1344.992688	148912.878168	36.013376
1346.465104	149160.485557	36.018394
1347.706908	149412.584477	36.023412
1348.762947	149667.252442	36.028429
1350.303306	149916.083895	36.033447
1351.500103	150172.723314	36.038464
1352.916903	150423.481061	36.043482
1354.283000	150682.315586	36.048500
1355.532947	150951.102359	36.053517
1356.752270	151206.375269	36.058535
1358.114460	151471.747957	36.063552
1359.283698	151729.353799	36.068570
1360.847266	152004.006893	36.073588
1362.039866	152277.746598	36.078605
1363.308045	152540.465926	36.083623
1364.879440	152815.618235	36.088640
1366.702103	153086.481737	36.093658
1368.176521	153362.161353	36.098676
1369.013025	153638.531843	36.103693
1370.804594	153901.351532	36.108711
1372.138721	154185.305176	36.113728
1373.381506	154448.713956	36.118746
1374.980642	154721.972501	36.123764
1376.371983	155010.933212	36.128781
1377.715491	155284.770691	36.133799
1378.763251	155561.690695	36.138816
1380.227969	155840.408463	36.143834
1381.788069	156120.139941	36.148852
1382.898571	156413.406904	36.153869
1384.451153	156683.642220	36.158887
1385.656943	156977.519172	36.163904
1387.025204	157272.804913	36.168922
1388.506792	157563.735563	36.173940
1389.755381	157843.200744	36.178957
1391.128009	158138.238390	36.183975
1392.735457	158429.496998	36.188992
1394.279126	158713.600569	36.194010
1395.693795	159008.688334	36.199028
1396.908479	159305.029164	36.204045
1398.595661	159599.809745	36.209063
1400.042450	159879.002405	36.214080
1401.247603	160175.820487	36.219098
1402.933751	160465.976830	36.224116
1404.053083	160760.593116	36.229133
1405.385272	161057.206209	36.234151
1407.429153	161354.845628	36.239168
1408.725800	161640.025112	36.244186
1410.192448	161936.901335	36.249204
1411.267232	162221.233324	36.254221
1412.821343	162511.679416	36.259239
1414.083371	162808.684390	36.264256
1415.701440	163097.664876	36.269274
1417.055485	163381.463680	36.274292
1418.198587	163677.974174	36.279309
1419.985928	163973.796622	36.284327
1421.410713	164270.505724	36.289344
1422.894213	164562.702960	36.294362
1424.604121	164849.916442	36.299380
1425.932999	165142.320767	36.304397
1427.642612	165435.019408	36.309415
1428.387119	165719.746331	36.314432
1429.882419	166016.760211	36.319450
1431.567359	166300.256989	36.324468
1432.775208	166582.197611	36.329485
1434.213368	166853.012171	36.334503
1435.511834	167132.517806	36.339520
1436.985383	167407.745544	36.344538
1438.614343	167682.226038	36.349556
1439.716865	167968.836945	36.354573
1441.634040	168236.979527	36.359591
1442.749115	168518.554349	36.364608
1444.415732	168798.973901	36.369626
1445.794056	169072.248057	36.374644
1446.795013	169355.648797	36.379661
1448.264278	169638.910466	36.384679
1450.019080	169939.625421	36.389696
1451.112053	170231.962425	36.394714
1452.901920	170511.191994	36.399732
1454.213657	170811.325991	36.404749
1455.693438	171097.500823	36.409767
1457.120104	171393.838050	36.414784
1458.312678	171698.857663	36.419802
1459.931959	171998.174397	36.424820
1461.149873	172306.036324	36.429837
1462.957752	172599.805538	36.434855
1463.845422	172901.824994	36.439872
1465.256976	173215.155702	36.444890
1466.857880	173519.929235	36.449908
1468.153471	173844.526921	36.454925
1469.965078	174153.000663	36.459943
1471.421659	174469.149426	36.464960
1472.621236	174788.591546	36.469978
1474.396338	175101.811008	36.474996
1475.962295	175429.623492	36.480013
1477.354633	175744.077877	36.485031
1479.042573	176069.336284	36.490048
1480.180958	176385.841914	36.495066
1481.792584	176701.839869	36.500084
1483.074519	177031.144027	36.505101
1484.849595	177357.665607	36.510119
1486.022087	177678.285815	36.515136
1487.954559	178002.805713	36.520154
1489.363289	178326.094304	36.525172
1490.870702	178660.410439	36.530189
1492.563518	178991.271347	36.535207
1494.083955	179318.126860	36.540224
1495.497375	179638.706924	36.545242
1497.029644	179957.936679	36.550260
1498.562591	180288.083506	36.555277
1499.876769	180614.727452	36.560295
1501.770439	180935.883476	36.565312
1503.131852	181270.329456	36.570330
1504.729685	181594.356085	36.575348
1505.946290	181924.387782	36.580365
1508.121576	182259.390935	36.585383
1509.444380	182584.763690	36.590400
1510.989503	182915.305711	36.595418
1512.464694	183243.754308	36.600436
1513.705734	183575.708749	36.605453
1515.574843	183914.694898	36.610471
1517.192871	184231.257934	36.615488
1518.364230	184562.544466	36.620506
1520.269589	184890.043382	36.625524
1521.801143	185215.993954	36.630541
1523.130226	185539.009647	36.635559
1524.924710	185869.172875	36.640576
1526.063696	186191.627156	36.645594
1528.045334	186509.945584	36.650612
1529.418580	186847.444872	36.655629
1530.775591	187170.478007	36.660647
1532.628723	187488.048835	36.665664
1533.760948	187797.362585	36.670682
1535.201138	188102.806244	36.675700
1536.508423	188416.499182	36.680717
1538.105016	188730.514143	36.685735
1539.690349	189035.316717	36.690752
1541.137716	189360.822516	36.695770
1542.428584	189668.469752	36.700788
1543.985452	189989.048245	36.705805
1545.317273	190306.631689	36.710823
1547.090292	190620.437145	36.715840
1548.559768	190967.858747	36.720858
1549.646734	191292.622196	36.725876
1551.157755	191631.230692	36.730893
1552.234402	191972.667596	36.735911
1553.995323	192312.216078	36.740928
1555.441319	192660.819143	36.745946
1557.024875	192998.331439	36.750964
1558.442219	193363.167348	36.755981
1559.965726	193717.070054	36.760999
1561.850661	194078.367111	36.766016
1563.222585	194438.595722	36.771034
1564.948930	194789.614493	36.776052
1566.354334	195154.970532	36.781069
1568.004996	195518.053727	36.786087
1569.576689	195874.080595	36.791104
1570.912817	196241.142725	36.796122
1572.835721	196610.979196	36.801140
1574.681295	196978.177111	36.806157
1576.105150	197341.371380	36.811175
1577.918554	197717.554646	36.816192
1579.193793	198081.285327	36.821210
1580.673099	198452.589178	36.826228
1582.735963	198824.039879	36.831245
1583.893726	199183.834702	36.836263
1586.126220	199561.698340	36.841280
1587.483189	199932.509887	36.846298
1589.392646	200298.001234	36.851316
1590.645741	200671.855608	36.856333
1592.122797	201041.205799	36.861351
1593.993717	201416.003157	36.866368
1595.452957	201787.099597	36.871386
1597.562241	202153.430876	36.876404
1599.310939	202533.980476	36.881421
1600.767020	202910.047641	36.886439
1602.575672	203271.025368	36.891456
1603.893646	203662.952227	36.896474
1605.864590	204017.367853	36.901492
1607.399928	204389.823495	36.906509
1609.025210	204760.501218	36.911527
1610.686023	205130.920941	36.916544
1611.811483	205500.846830	36.921562
1613.526792	205880.961893	36.926580
1615.321911	206249.015815	36.931597
1616.838501	206629.319740	36.936615
1618.730729	206992.751946	36.941632
1620.082029	207382.990876	36.946650
1621.941464	207759.802560	36.951668
1623.382374	208131.161658	36.956685
1624.818886	208508.160990	36.961703
1626.714532	208883.918021	36.966720
1628.044162	209269.090513	36.971738
1630.119238	209642.637332	36.976756
1631.291345	210019.877732	36.981773
1632.990434	210404.676991	36.986791
1634.720561	210782.133371	36.991808
1635.958701	211174.529537	36.996826
1637.722803	211547.463135	37.001844
1639.359731	211927.174823	37.006861
1641.066386	212296.997350	37.011879
1642.867477	212650.323345	37.016896
1644.451361	213010.391394	37.021914
1646.011782	213379.404493	37.026932
1647.372999	213741.315438	37.031949
1649.021627	214107.878817	37.036967
1650.581270	214482.534688	37.041984
1652.272511	214852.217853	37.047002
1653.872751	215222.222288	37.052020
1655.649048	215604.288331	37.057037
1656.751817	215982.682922	37.062055
1658.332615	216356.911004	37.067072
1659.828347	216756.425456	37.072090
1661.633871	217142.658033	37.077108
1663.199319	217530.811240	37.082125
1664.633642	217931.712102	37.087143
1666.035871	218334.397747	37.092160
1667.648791	218738.218512	37.097178
1669.477485	219137.636693	37.102196
1671.237922	219562.390059	37.107213
1672.578533	219985.512791	37.112231
1674.199843	220387.586069	37.117248
1676.101099	220820.982214	37.122266
1677.675606	221238.127937	37.127284
1679.533918	221664.676824	37.132301
1681.084484	222091.684580	37.137319
1682.862550	222510.503227	37.142336
1684.617749	222941.645888	37.147354
1686.107169	223380.250714	37.152372
1688.040150	223814.643806	37.157389
1689.543318	224260.463143	37.162407
1691.088962	224751.387069	37.167424
1692.733712	225199.040697	37.172442
1694.299887	225640.028763	37.177460
1696.452971	226077.873452	37.182477
1697.853242	226525.419860	37.187495
1699.885814	226969.434372	37.192512
1701.444762	227418.862706	37.197530
1703.244071	227861.039176	37.202548
1704.814040	228303.280402	37.207565
1706.341076	228758.205038	37.212583
1708.151272	229205.946842	37.217600
1709.805319	229663.596756	37.222618
1711.658166	230119.589668	37.227636
1713.367212	230572.813689	37.232653
1714.787449	231040.412957	37.237671
1716.954122	231494.402467	37.242688
1718.902098	231955.262365	37.247706
1720.420272	232409.209321	37.252724
1722.466850	232861.876462	37.257741
1724.102551	233314.155539	37.262759
1725.543269	233770.202094	37.267776
1727.780180	234232.519572	37.272794
1729.646407	234689.489030	37.277812
1731.387774	235137.996203	37.282829
1733.137622	235596.257370	37.287847
1735.073239	236038.511353	37.292864
1736.803736	236492.231102	37.297882
1738.571537	236946.936476	37.302900
1740.734757	237398.199184	37.307917
1741.855732	237857.255688	37.312935
1743.492999	238289.708275	37.317952
1745.579566	238746.194155	37.322970
1747.314711	239199.081186	37.327988
1749.400624	239650.082299	37.333005
1751.036379	240104.715024	37.338023
1752.759768	240539.622034	37.343040
1754.427882	240987.621216	37.348058
1756.520294	241420.792398	37.353076
1758.050598	241829.493061	37.358093
1759.158025	242267.705723	37.363111
1761.576243	242688.936994	37.368128
1763.138497	243121.309643	37.373146
1764.806881	243549.220017	37.378164
1766.623080	243967.707677	37.383181
1767.992004	244406.185538	37.388199
1769.758213	244836.749013	37.393216
1771.423298	245273.578893	37.398234
1772.939185	245726.412394	37.403252
1774.570178	246172.699005	37.408269
1776.093196	246627.590222	37.413287
1778.007715	247073.831210	37.418304
1779.740349	247538.367504	37.423322
1781.577257	247998.136809	37.428340
1783.570653	248463.240849	37.433357
1784.980896	248927.882875	37.438375
1786.774493	249399.803578	37.443392
1788.776001	249870.445696	37.448410
1790.246146	250340.083715	37.453428
1792.322566	250807.843832	37.458445
1794.274028	251290.714471	37.463463
1796.150588	251759.067292	37.468480
1797.527558	252239.620309	37.473498
1799.266806	252721.739660	37.478516
1801.694426	253193.279534	37.483533
1803.067346	253683.080994	37.488551
1804.985336	254171.827399	37.493568
1807.090432	254654.039931	37.498586
1808.769244	255149.609001	37.503604
1810.721310	255636.496036	37.508621
1812.613501	256113.739885	37.513639
1814.614080	256603.464395	37.518656
1816.327723	257092.347296	37.523674
1818.338971	257574.449263	37.528692
1820.223503	258064.828291	37.533709
1821.728091	258559.563259	37.538727
1823.559372	259046.902722	37.543744
1825.633549	259531.255264	37.548762
1827.004173	260030.889716	37.553780
1829.325216	260525.870739	37.558797
1831.017476	261023.953078	37.563815
1832.929964	261525.225119	37.568832
1834.604253	262025.062930	37.573850
1836.612159	262516.106717	37.578868
1838.696316	263010.135265	37.583885
1840.396829	263519.062396	37.588903
1842.530613	264017.502346	37.593920
1844.376889	264509.587843	37.598938
1846.233032	265011.604006	37.603956
1847.915703	265500.489587	37.608973
1849.930781	266001.996036	37.613991
1851.847011	266492.366389	37.619008
1853.730567	266978.448553	37.624026
1855.339220	267482.256164	37.629044
1857.859864	267968.155897	37.634061
1859.113978	268468.413720	37.639079
1861.200775	268961.623822	37.644096
1863.332648	269466.130174	37.649114
1865.336522	269965.678019	37.654132
1867.192477	270459.914996	37.659149
1869.051772	270947.317353	37.664167
1871.069561	271434.896042	37.669184
1872.833341	271923.735264	37.674202
1874.579235	272420.527713	37.679220
1876.609152	272908.635518	37.684237
1878.422923	273394.542752	37.689255
1880.033678	273865.520537	37.694272
1882.237998	274332.258862	37.699290
1883.774469	274801.723092	37.704308
1885.760829	275262.653144	37.709325
1887.437973	275737.680917	37.714343
1889.421341	276204.553830	37.719360
1891.192316	276672.781797	37.724378
1893.052715	277161.290419	37.729396
1894.601513	277628.511580	37.734413
1896.320484	278116.711183	37.739431
1897.989264	278607.839176	37.744448
1900.396536	279090.944017	37.749466
1901.758171	279585.930651	37.754484
1903.841456	280080.974675	37.759501
1905.765688	280585.569354	37.764519
1907.609758	281090.175901	37.769536
1909.462887	281596.252850	37.774554
1911.023620	282106.872723	37.779572
1913.248186	282626.297412	37.784589
1915.163501	283140.818302	37.789607
1916.738003	283661.236194	37.794624
1918.819671	284178.063302	37.799642
1920.311254	284708.652021	37.804660
1922.344958	285233.053158	37.809677
1924.379131	285760.297341	37.814695
1926.388589	286298.186747	37.819712
1928.184733	286832.223089	37.824730
1930.059577	287373.559879	37.829748
1932.415382	287909.201647	37.834765
1934.318109	288445.068576	37.839783
1936.368006	288989.037248	37.844800
1938.374070	289520.488593	37.849818
1939.971373	290067.423238	37.854836
1942.058379	290616.459132	37.859853
1943.990412	291163.003653	37.864871
1945.994721	291712.810448	37.869888
1948.287160	292247.225745	37.874906
1949.957988	292809.223781	37.879924
1951.868494	293355.660470	37.884941
1953.775210	293908.927695	37.889959
1955.915028	294460.807623	37.894976
1958.279943	295012.876304	37.899994
1960.052464	295571.389850	37.905012
1962.107190	296112.430308	37.910029
1964.074219	296672.480868	37.915047
1966.203106	297225.161564	37.920064
1968.295962	297771.597281	37.925082
1969.893254	298341.453096	37.930100
1972.212587	298885.610482	37.935117
1974.401666	299442.815696	37.940135
1976.138706	299990.415811	37.945152
1978.369451	300537.778986	37.950170
1980.468447	301098.062870	37.955188
1982.568462	301646.609653	37.960205
1984.746596	302202.988165	37.965223
1986.640464	302744.781491	37.970240
1988.989616	303292.058441	37.975258
1990.696554	303841.520699	37.980276
1992.667976	304377.932786	37.985293
1994.525434	304928.684172	37.990311
1996.238702	305477.297224	37.995328
1998.787754	306032.981385	38.000346
2000.474631	306594.924783	38.005364
2002.253235	307140.291145	38.010381
2004.374583	307699.742856	38.015399
2005.973866	308254.883554	38.020416
2008.204998	308811.236750	38.025434
2010.017894	309371.718442	38.030452
2012.118475	309904.620414	38.035469
2014.013986	310439.355719	38.040487
2015.531299	310970.442198	38.045504
2018.014496	311499.308627	38.050522
2019.622244	312040.632275	38.055540
2021.995186	312582.816129	38.060557
2023.873841	313129.750215	38.065575
2025.394587	313679.126423	38.070592
2027.385022	314226.719639	38.075610
2029.497690	314788.026474	38.080628
2031.509458	315339.289884	38.085645
2033.269832	315909.406870	38.090663
2035.035648	316476.801357	38.095680
2037.150096	317040.274032	38.100698
2038.872919	317623.714532	38.105716
2040.864512	318212.742823	38.110733
2043.031764	318793.535415	38.115751
2045.042708	319384.404007	38.120768
2047.182533	319969.456837	38.125786
2049.115920	320569.849607	38.130804
2050.985022	321158.796112	38.135821
2053.436293	321762.342530	38.140839
2055.013818	322359.248253	38.145856
2057.392666	322965.842218	38.150874
2059.489574	323578.215112	38.155892
2061.576749	324183.398290	38.160909
2063.802766	324801.831473	38.165927
2065.250488	325417.670274	38.170944
2067.670683	326020.317672	38.175962
2069.839964	326648.084753	38.180980
2072.081410	327271.314171	38.185997
2074.280419	327892.563765	38.191015
2075.960077	328521.178937	38.196032
2078.490191	329136.775303	38.201050
2080.362265	329764.634402	38.206068
2082.658143	330390.563391	38.211085
2084.766095	331021.720849	38.216103
2086.686459	331660.568998	38.221120
2089.153107	332288.530424	38.226138
2091.078809	332922.133596	38.231156
2093.269729	333555.634903	38.236173
2095.238026	334186.297023	38.241191
2097.364020	334824.566704	38.246208
2099.539817	335467.339075	38.251226
2101.783571	336106.640133	38.256244
2104.233777	336740.644789	38.261261
2106.386593	337376.594642	38.266279
2107.984057	338016.664375	38.271296
2109.980877	338646.100716	38.276314
2112.169841	339299.509956	38.281332
2114.039986	339942.581839	38.286349
2116.467370	340584.868163	38.291367
2118.758230	341240.418183	38.296384
2120.421323	341881.392476	38.301402
2122.858641	342540.124474	38.306420
2125.052349	343197.491797	38.311437
2127.084123	343830.232205	38.316455
2129.133932	344494.788275	38.321472
2131.560219	345140.364778	38.326490
2133.408064	345797.068084	38.331508
2135.432955	346443.987285	38.336525
2137.911831	347099.349864	38.341543
2139.812816	347751.651570	38.346560
2142.351959	348412.061181	38.351578
2144.125356	349068.933176	38.356596
2146.399872	349720.104452	38.361613
2148.582985	350370.063237	38.366631
2150.706916	351021.900163	38.371648
2153.078398	351654.705058	38.376666
2154.780423	352284.134803	38.381684
2157.161726	352916.945159	38.386701
2159.271173	353533.449438	38.391719
2160.989178	354164.067189	38.396736
2162.963443	354795.166185	38.401754
2165.231776	355434.961326	38.406772
2167.422009	356075.901455	38.411789
2169.612390	356717.719803	38.416807
2171.223922	357374.213249	38.421824
2173.412862	358016.214691	38.426842
2175.682701	358672.654867	38.431860
2177.382802	359340.189851	38.436877
2179.769957	359996.081825	38.441895
2181.565432	360679.740435	38.446912
2183.997308	361347.857039	38.451930
2186.635733	362024.833183	38.456948
2188.434919	362700.109606	38.461965
2190.786995	363379.570511	38.466983
2193.282672	364080.736837	38.472000
2195.291119	364755.689334	38.477018
2197.267339	365443.902652	38.482036
2199.463645	366136.785550	38.487053
2202.131560	366816.387147	38.492071
2203.970209	367520.972451	38.497088
2206.474019	368207.044380	38.502106
2208.685576	368905.809254	38.507124
2210.953486	369613.429352	38.512141
2213.330258	370303.414866	38.517159
2215.425114	371021.182091	38.522176
2217.656072	371716.389831	38.527194
2219.911796	372421.547727	38.532212
2222.119165	373133.953386	38.537229
2224.120974	373848.407660	38.542247
2226.598074	374570.681823	38.547264
2228.789266	375279.014422	38.552282
2230.803189	375997.328560	38.557300
2233.133111	376718.213096	38.562317
2235.600301	377440.733617	38.567335
2237.473087	378157.681978	38.572352
2239.934254	378880.325188	38.577370
2242.632031	379609.861941	38.582388
2244.433633	380345.794013	38.587405
2247.109755	381065.945848	38.592423
2249.234797	381794.971599	38.597440
2251.521293	382517.438237	38.602458
2253.999711	383247.387737	38.607476
2256.231745	383980.835134	38.612493
2258.466256	384709.296192	38.617511
2261.041994	385443.566444	38.622528
2263.180154	386175.204719	38.627546
2265.903177	386896.132500	38.632564
2268.095376	387625.041173	38.637581
2270.296591	388343.334812	38.642599
2272.696362	389077.676702	38.647616
2274.836764	389793.285275	38.652634
2277.636677	390522.837277	38.657652
2279.497647	391253.388825	38.662669
2281.787289	391962.686662	38.667687
2284.430977	392696.673958	38.672704
2286.667964	393404.020461	38.677722
2289.004397	394123.424089	38.682740
2291.115137	394851.414512	38.687757
2293.639308	395575.238409	38.692775
2295.811878	396303.005703	38.697792
2298.418567	397017.910188	38.702810
2300.660709	397735.670512	38.707828
2303.019692	398448.604194	38.712845
2305.648695	399135.247009	38.717863
2307.886693	399815.830803	38.722880
2310.178246	400492.917992	38.727898
2312.619340	401169.229630	38.732916
2314.786060	401847.014848	38.737933
2317.207086	402526.540960	38.742951
2319.279394	403203.777143	38.747968
2321.271471	403895.934105	38.752986
2323.962940	404572.046878	38.758004
2325.949216	405275.445529	38.763021
2328.471890	405948.866967	38.768039
2330.925745	406655.092276	38.773056
2333.031156	407339.493272	38.778074
2335.445455	408023.648803	38.783092
2337.605252	408730.603635	38.788109
2339.921938	409425.278497	38.793127
2342.057853	410142.257293	38.798144
2344.479794	410860.030961	38.803162
2346.980231	411565.892358	38.808180
2349.534070	412273.372605	38.813197
2352.167124	412985.886654	38.818215
2354.314729	413705.426822	38.823232
2356.677267	414419.922174	38.828250
2359.420924	415144.389868	38.833268
2361.490985	415867.200953	38.838285
2363.797937	416582.430994	38.843303
2366.009309	417317.384992	38.848320
2368.481967	418033.281614	38.853338
2370.707462	418770.242677	38.858356
2373.039120	419516.204988	38.863373
2375.515027	420242.902054	38.868391
2378.138431	420983.910873	38.873408
2380.342423	421717.801224	38.878426
2382.931390	422457.278007	38.883444
2385.395535	423204.905998	38.888461
2388.117707	423938.796899	38.893479
2390.325615	424678.168628	38.898496
2392.599444	425416.696957	38.903514
2395.174787	426159.304900	38.908532
2397.723916	426915.665793	38.913549
2400.133075	427660.735847	38.918567
2402.482290	428404.020693	38.923584
2405.073455	429156.101928	38.928602
2407.467870	429898.320171	38.933620
2410.135644	430653.277457	38.938637
2412.590754	431394.173093	38.943655
2415.010876	432144.314381	38.948672
2417.648147	432889.587081	38.953690
2420.190998	433627.157862	38.958708
2422.270969	434372.424259	38.963725
2424.871471	435120.161908	38.968743
2427.311618	435870.229749	38.973760
2429.565910	436614.179918	38.978778
2432.484192	437355.769467	38.983796
2434.930130	438101.562358	38.988813
2437.315184	438856.196377	38.993831
2439.848524	439586.744373	38.998848
2442.181729	440327.775917	39.003866
2444.867713	441072.367745	39.008884
2447.153607	441808.854397	39.013901
2449.838294	442554.509731	39.018919
2452.489321	443293.163363	39.023936
2454.907194	444046.198796	39.028954
2457.757221	444772.779216	39.033972
2459.786641	445511.662680	39.038989
2462.408728	446245.920876	39.044007
2464.948037	446976.070297	39.049024
2467.433027	447707.367281	39.054042
2470.304664	448400.790640	39.059060
2472.512472	449095.413728	39.064077
2474.830654	449788.073885	39.069095
2477.334252	450487.407532	39.074112
2479.484177	451189.810851	39.079130
2481.906822	451876.164356	39.084148
2484.130802	452592.213955	39.089165
2486.483883	453296.384187	39.094183
2489.255021	454008.198566	39.099200
2491.539700	454723.254423	39.104218
2494.018541	455433.702573	39.109236
2496.451700	456158.089169	39.114253
2498.514197	456876.747249	39.119271
2501.144153	457607.016235	39.124288
2503.812911	458345.089031	39.129306
2506.399851	459073.846071	39.134324
2508.835861	459809.628698	39.139341
2510.831056	460550.765089	39.144359
2513.686966	461295.118900	39.149376
2515.551972	462049.920298	39.154394
2518.659299	462803.729839	39.159412
2520.838481	463566.256369	39.164429
2523.123758	464325.905489	39.169447
2525.795699	465087.331424	39.174464
2528.182250	465869.293538	39.179482
2530.914073	466642.929805	39.184500
2533.711870	467426.277538	39.189517
2535.982032	468226.002610	39.194535
2538.791004	469003.422662	39.199552
2541.224196	469793.101092	39.204570
2543.856202	470564.423516	39.209588
2546.256051	471362.834042	39.214605
2548.616881	472150.658244	39.219623
2551.802210	472948.821747	39.224640
2554.215858	473749.857181	39.229658
2556.648731	474533.326232	39.234676
2559.202281	475347.404295	39.239693
2562.067374	476142.200996	39.244711
2564.637491	476943.477457	39.249728
2567.091484	477754.334642	39.254746
2569.755250	478547.444782	39.259764
2572.291128	479366.500047	39.264781
2574.657305	480172.517469	39.269799
2577.529268	480981.041634	39.274816
2579.848957	481808.253789	39.279834
2582.816261	482610.124928	39.284852
2585.558528	483428.558573	39.289869
2587.737305	484253.964770	39.294887
2590.500634	485058.940747	39.299904
2592.835848	485891.969708	39.304922
2595.796620	486704.007266	39.309940
2598.051126	487529.753469	39.314957
2600.327419	488364.492730	39.319975
2603.514135	489184.404340	39.324992
2605.905781	490016.824809	39.330010
2608.668273	490845.661829	39.335028
2611.152447	491680.712624	39.340045
2613.489105	492516.655735	39.345063
2616.469251	493345.538680	39.350080
2618.898308	494179.619381	39.355098
2621.770768	495010.205523	39.360116
2624.123420	495845.529200	39.365133
2626.523269	496698.815574	39.370151
2629.592482	497520.820614	39.375168
2631.727757	498371.493000	39.380186
2634.478726	499208.400465	39.385204
2637.470542	500052.540460	39.390221
2639.992046	500882.238902	39.395239
2642.733180	501697.535319	39.400256
2644.845484	502513.046552	39.405274
2647.494466	503313.097346	39.410292
2650.016025	504113.684897	39.415309
2652.675526	504931.809808	39.420327
2655.200686	505753.496013	39.425344
2657.860193	506579.706964	39.430362
2660.254289	507386.608644	39.435380
2663.013397	508225.525741	39.440397
2665.758872	509050.839720	39.445415
2668.142782	509879.548459	39.450432
2670.824573	510722.128538	39.455450
2673.456689	511551.919242	39.460468
2675.979216	512400.233404	39.465485
2678.386074	513263.641589	39.470503
2681.393132	514117.277283	39.475520
2683.611550	514983.293265	39.480538
2686.274156	515852.665173	39.485556
2689.345179	516717.889995	39.490573
2691.720037	517597.592289	39.495591
2694.404410	518477.495847	39.500608
2697.059034	519372.418268	39.505626
2699.520250	520251.451144	39.510644
2702.444089	521132.724936	39.515661
2704.986735	522048.314723	39.520679
2708.003196	522939.492922	39.525696
2710.374632	523855.858216	39.530714
2712.969678	524763.921707	39.535732
2715.941818	525670.508454	39.540749
2718.836002	526587.376581	39.545767
2721.777127	527512.791340	39.550784
2724.206601	528432.694283	39.555802
2727.422385	529355.582439	39.560820
2729.776481	530275.433675	39.565837
2732.365820	531200.675957	39.570855
2735.743726	532125.880864	39.575872
2738.441121	533058.740155	39.580890
2740.956326	533986.838523	39.585908
2744.046411	534923.791697	39.590925
2746.633284	535871.033683	39.595943
2749.403133	536799.010326	39.600960
2752.193229	537742.271113	39.605978
2754.720902	538676.204558	39.610996
2757.638770	539623.647279	39.616013
2760.427227	540566.419734	39.621031
2763.348017	541514.490372	39.626048
2765.916649	542458.028176	39.631066
2768.865606	543410.946541	39.636084
2771.530833	544358.414969	39.641101
2774.504866	545317.788102	39.646119
2777.488195	546277.445605	39.651136
2780.492560	547232.406986	39.656154
2782.847059	548177.302889	39.661172
2786.116130	549124.547369	39.666189
2788.895777	550090.509524	39.671207
2791.476115	551026.977240	39.676224
2794.550584	551994.565890	39.681242
2797.191413	552938.784178	39.686260
2799.976303	553883.867838	39.691277
2803.047841	554840.145978	39.696295
2806.148940	555781.576614	39.701312
2808.641443	556742.036132	39.706330
2811.279833	557694.765058	39.711348
2814.803962	558650.495314	39.716365
2817.338795	559596.372459	39.721383
2819.723218	560536.379410	39.726400
2822.635735	561498.987503	39.731418
2825.330069	562423.337047	39.736436
2828.260020	563351.449844	39.741453
2830.799581	564270.621594	39.746471
2833.478320	565185.286289	39.751488
2836.137332	566098.785033	39.756506
2839.135103	567019.544409	39.761524
2841.972640	567942.172324	39.766541
2844.514609	568860.214200	39.771559
2847.307590	569797.977963	39.776576
2850.068653	570734.724399	39.781594
2852.622826	571669.227543	39.786612
2855.553845	572613.185836	39.791629
2858.266545	573570.107661	39.796647
2861.123216	574522.768072	39.801664
2863.898337	575486.509145	39.806682
2866.632592	576445.265803	39.811700
2869.763902	577420.389255	39.816717
2871.944892	578392.733570	39.821735
2875.111110	579374.370004	39.826752
2878.308795	580353.214802	39.831770
2880.958418	581336.836871	39.836788
2884.124384	582332.481481	39.841805
2886.446998	583328.785967	39.846823
2889.482475	584327.498977	39.851840
2892.301189	585325.564109	39.856858
2895.390242	586335.133480	39.861876
2898.351134	587353.713047	39.866893
2901.289311	588364.140149	39.871911
2904.160753	589382.813279	39.876928
2907.190045	590405.633591	39.881946
2910.462983	591423.665623	39.886964
2913.424144	592440.409218	39.891981
2916.340617	593471.903600	39.896999
2919.472632	594492.851784	39.902016
2922.801201	595509.972037	39.907034
2925.626254	596543.015920	39.912052
2928.968701	597558.002601	39.917069
2931.640108	598583.228241	39.922087
2934.617738	599617.126566	39.927104
2937.888160	600635.612199	39.932122
2941.098253	601669.188658	39.937140
2944.151835	602678.567389	39.942157
2946.735948	603714.816648	39.947175
2949.878624	604728.655621	39.952192
2952.974927	605762.882718	39.957210
2955.787194	606784.651202	39.962228
2959.092863	607810.900059	39.967245
2961.871382	608839.043997	39.972263
2965.225028	609862.296227	39.977280
2968.243677	610886.661052	39.982298
2971.411026	611905.605157	39.987316
2974.557116	612925.059926	39.992333
2977.154009	613948.562925	39.997351
2980.711371	614958.360605	40.002368
2983.714981	615971.957684	40.007386
2986.393442	616995.365166	40.012404
2989.770393	618008.913047	40.017421
2992.971367	619033.694064	40.022439
2996.009188	620041.660457	40.027456
2999.076874	621047.829231	40.032474
3002.199959	622069.038587	40.037492
3005.274187	623067.622187	40.042509
3008.192599	624087.924892	40.047527
3011.050799	625086.556834	40.052544
3014.131254	626095.500407	40.057562
3016.859634	627101.709347	40.062580
3020.191937	628105.476077	40.067597
3022.942494	629121.630033	40.072615
3025.738851	630118.652200	40.077632
3028.890195	631092.152412	40.082650
3031.273098	632072.629648	40.087668
3034.834068	633026.660303	40.092685
3037.363572	634015.119650	40.097703
3040.090243	634981.140530	40.102720
3042.944991	635970.958315	40.107738
3045.874116	636953.083749	40.112756
3048.654745	637940.579881	40.117773
3051.600104	638943.123191	40.122791
3054.493950	639946.675069	40.127808
3057.626485	640965.454842	40.132826
3060.050443	641989.138566	40.137844
3063.203709	643017.637079	40.142861
3065.717726	644054.615370	40.147879
3068.559685	645096.171086	40.152896
3071.878865	646154.743316	40.157914
3074.571826	647213.706624	40.162932
3077.938621	648273.942981	40.167949
3080.708258	649355.150901	40.172967
3083.755875	650428.171841	40.177984
3086.745904	651516.436073	40.183002
3089.509881	652619.019245	40.188020
3093.074816	653713.923994	40.193037
3095.761273	654816.723590	40.198055
3098.805144	655923.574968	40.203072
3102.302065	657048.805063	40.208090
3105.030641	658172.887100	40.213108
3108.005870	659294.558277	40.218125
3110.838398	660430.612612	40.223143
3113.940907	661571.169160	40.228160
3117.255804	662719.520735	40.233178
3120.149731	663873.827396	40.238196
3123.864860	665028.855428	40.243213
3126.714032	666200.506872	40.248231
3129.768395	667358.049689	40.253248
3133.216682	668525.883711	40.258266
3136.576764	669704.332841	40.263284
3139.502456	670872.113151	40.268301
3142.841163	672045.499193	40.273319
3146.069900	673215.176892	40.278336
3149.257987	674390.830562	40.283354
3152.397257	675572.806797	40.288372
3155.913274	676743.089270	40.293389
3159.179305	677922.409954	40.298407
3162.318861	679106.918307	40.303424
3165.750738	680275.724631	40.308442
3168.694226	681457.379571	40.313460
3171.952304	682633.962545	40.318477
3175.277829	683827.120568	40.323495
3178.925392	685000.553079	40.328512
3182.155751	686169.136130	40.333530
3185.076312	687353.109408	40.338548
3188.559817	688532.367109	40.343565
3191.705446	689703.237223	40.348583
3194.734219	690892.633850	40.353600
3198.451879	692059.826497	40.358618
3201.434134	693244.848876	40.363636
3204.913091	694411.822397	40.368653
3207.997548	695592.099763	40.373671
3211.357122	696753.923472	40.378688
3214.740892	697933.838542	40.383706
3217.485491	699114.394756	40.388724
3220.803927	700274.867524	40.393741
3224.051969	701459.535772	40.398759
3227.214869	702637.415784	40.403776
3230.395678	703814.290735	40.408794
3233.402673	704991.579481	40.413812
3237.291838	706157.118357	40.418829
3240.209247	707290.561208	40.423847
3243.156317	708432.170303	40.428864
3246.652382	709555.708975	40.433882
3249.636983	710677.748162	40.438900
3252.568818	711805.044632	40.443917
3255.851886	712947.281146	40.448935
3258.905106	714088.609531	40.453952
3261.781223	715242.432388	40.458970
3264.845194	716390.128384	40.463988
3267.829221	717549.455686	40.469005
3271.032238	718719.568244	40.474023
3274.046439	719903.001277	40.479040
3277.645671	721078.652667	40.484058
3280.176648	722275.971268	40.489076
3283.774786	723470.122748	40.494093
3286.696470	724679.042602	40.499111
3289.834498	725889.133090	40.504128
3293.283731	727095.583973	40.509146
3296.116150	728336.644643	40.514164
3299.202136	729558.602815	40.519181
3302.388798	730807.380025	40.524199
3305.625611	732059.018652	40.529216
3308.937827	733319.833225	40.534234
3311.978031	734594.714533	40.539252
3315.477023	735860.383004	40.544269
3318.941556	737147.820757	40.549287
3322.180201	738429.857225	40.554304
3325.639273	739716.732976	40.559322
3329.020840	741014.463289	40.564340
3332.044584	742303.309322	40.569357
3335.642303	743609.258815	40.574375
3339.142709	744918.656242	40.579392
3342.414959	746217.914023	40.584410
3345.618935	747537.768079	40.589428
3349.086557	748851.046891	40.594445
3352.802930	750165.048167	40.599463
3355.693198	751492.018176	40.604480
3359.300381	752821.400420	40.609498
3362.547643	754158.984711	40.614516
3365.949238	755485.132756	40.619533
3369.656040	756826.410225	40.624551
3372.731806	758159.975327	40.629568
3376.441805	759491.823971	40.634586
3380.043864	760844.172076	40.639604
3383.407832	762171.079131	40.644621
3386.462591	763510.297288	40.649639
3389.832900	764867.568660	40.654656
3393.685726	766214.532753	40.659674
3397.022471	767564.681752	40.664692
3400.353733	768906.672996	40.669709
3403.963981	770251.864690	40.674727
3407.196507	771602.131355	40.679744
3411.050823	772943.058160	40.684762
3414.593352	774293.320389	40.689780
3418.009248	775630.832071	40.694797
3421.858736	776968.812998	40.699815
3424.936469	778308.835226	40.704832
3428.727828	779646.971073	40.709850
3432.106289	780988.706131	40.714868
3435.718580	782331.821373	40.719885
3439.471290	783667.451887	40.724903
3442.417159	784994.334836	40.729920
3445.850960	786324.078598	40.734938
3449.182596	787666.142006	40.739956
3453.055217	788997.814507	40.744973
3456.750099	790323.483224	40.749991
3460.107173	791658.366731	40.755008
3463.240042	792967.384723	40.760013
3466.645516	794231.907011	40.765018
3469.950378	795456.056189	40.770023
3473.532448	796608.029887	40.775028
3476.612168	797714.839343	40.780032
3479.934514	798719.260586	40.785037
3482.840347	799666.932124	40.790042
3485.581381	800544.736093	40.795047
3488.659069	801346.484273	40.800052
3491.303558	802095.481629	40.805056
3493.918808	802769.019632	40.810061
3496.094185	803367.874560	40.815066
3498.278943	803906.850229	40.820071
3500.427451	804386.507579	40.825076
3502.412681	804823.305332	40.830080
3504.471505	805180.637558	40.835085
3506.245680	805507.552899	40.840090
3507.549353	805775.407282	40.845095
3509.261296	805981.464668	40.850100
3510.613682	806153.015061	40.855104
3511.990582	806276.664218	40.860109
3513.180257	806365.930110	40.865114
3514.443603	806417.388757	40.870119
3515.587993	806418.866913	40.875124
3516.538358	806412.582933	40.880128
3517.305328	806363.485914	40.885133
3518.206373	806283.679715	40.890138
3519.069950	806172.799355	40.895143
3519.874410	806045.357467	40.900148
3520.514185	805897.693778	40.905152
3521.211377	805711.043027	40.910157
3521.533897	805515.673276	40.915162
3522.439756	805284.902048	40.920167
3523.009937	805049.030281	40.925172
3523.215139	804800.854709	40.930176
3523.628849	804521.205667	40.935181
3523.789266	804243.891606	40.940186
3524.003622	803955.720256	40.945191
3524.793638	803640.519409	40.950196
3524.606138	803330.271240	40.955200
3524.999491	803000.148691	40.960205
3525.415521	802670.938449	40.965210
3525.664727	802326.044379	40.970215
3525.415399	801966.107400	40.975220
3525.653414	801614.655755	40.980224
3526.265010	801245.170037	40.985229
3526.229137	800876.310884	40.990234
3526.035830	800495.830360	40.995239
3526.278625	800103.825030	41.000244
3526.464897	799727.900876	41.005248
3526.610694	799317.614021	41.010253
3526.454008	798933.901168	41.015258
3526.756108	798524.866651	41.020263
3526.549358	798121.977634	41.025268
3526.446223	797718.851872	41.030272
3526.452578	797299.732326	41.035277
3525.992204	796903.931795	41.040282
3526.104491	796497.067376	41.045287
3526.448710	796087.244545	41.050292
3526.028298	795682.825989	41.055296
3525.971982	795266.245788	41.060301
3526.123853	794854.271129	41.065306
3525.917293	794450.777245	41.070311
3526.219647	794025.028911	41.075316
3525.152332	793618.780735	41.080320
3525.725428	793199.518484	41.085325
3525.634081	792786.381977	41.090330
3525.216000	792377.793973	41.095335
3525.230398	791969.356606	41.100340
3525.103268	791553.943200	41.105344
3525.190036	791152.766168	41.110349
3525.214968	790750.250015	41.115354
3524.754863	790335.458463	41.120359
3524.975027	789931.045580	41.125364
3524.468196	789535.132087	41.130368
3524.734693	789124.523193	41.135373
3524.417659	788728.091074	41.140378
3524.476355	788325.038357	41.145383
3524.561542	787919.402622	41.150388
3524.163161	787523.113257	41.155392
3524.280954	787120.326588	41.160397
3523.948585	786724.276813	41.165402
3523.667479	786319.790087	41.170407
3523.418642	785921.273073	41.175412
3523.504491	785546.966801	41.180416
3523.466439	785144.536776	41.185421
3523.304344	784753.709062	41.190426
3523.005049	784370.258760	41.195431
3523.041765	783970.799254	41.200436
3522.427490	783593.703139	41.205440
3522.566946	783213.610459	41.210445
3522.495817	782824.728293	41.215450
3522.247875	782456.217821	41.220455
3522.226192	782073.730456	41.225460
3521.831784	781711.945042	41.230464
3521.816427	781331.630906	41.235469
3521.488396	780968.223004	41.240474
3521.279032	780606.253258	41.245479
3521.518563	780240.747250	41.250484
3520.983097	779881.747106	41.255488
3521.300009	779520.472797	41.260493
3520.817247	779158.032778	41.265498
3520.303840	778812.311837	41.270503
3520.545095	778459.215544	41.275508
3520.419413	778108.918693	41.280512
3520.479859	777756.457862	41.285517
3520.107388	777414.683158	41.290522
3519.845293	777070.905259	41.295527
3519.784778	776728.653163	41.300532
3519.312917	776395.756965	41.305536
3519.725065	776061.616846	41.310541
3519.219934	775732.437407	41.315546
3518.827164	775397.267159	41.320551
3519.234794	775062.786706	41.325556
3519.078727	774746.454805	41.330560
3518.658393	774413.213603	41.335565
3518.612192	774100.873553	41.340570
3518.255884	773785.567284	41.345575
3518.254911	773464.131390	41.350580
3518.492936	773165.888192	41.355584
3517.999053	772837.315552	41.360589
3518.187691	772534.228132	41.365594
3518.017576	772216.656668	41.370599
3517.876107	771904.337467	41.375604
3517.805837	771595.490812	41.380608
3517.551035	771294.888509	41.385613
3517.335401	770992.740299	41.390618
3517.261642	770695.384492	41.395623
3517.344539	770393.162574	41.400628
3517.057436	770099.710188	41.405632
3516.672792	769811.682224	41.410637
3516.626441	769519.497528	41.415642
3516.207447	769234.212138	41.420647
3516.477191	768938.848058	41.425652
3516.196626	768661.944452	41.430656
3516.054476	768370.913019	41.435661
3515.841019	768100.088393	41.440666
3515.356977	767825.207761	41.445671
3515.503591	767556.078284	41.450676
3515.419794	767290.920189	41.455680
3515.582029	767010.530445	41.460685
3515.297403	766758.399351	41.465690
3515.161859	766490.017248	41.470695
3515.309306	766222.564793	41.475700
3514.946382	765969.236815	41.480704
3514.981050	765705.481780	41.485709
3514.822510	765442.883208	41.490714
3514.667154	765195.706802	41.495719
3514.525249	764939.250704	41.500724
3514.387094	764689.195054	41.505728
3514.378751	764433.143380	41.510733
3514.154240	764191.812906	41.515738
3513.838844	763939.295952	41.520743
3514.085194	763690.475051	41.525748
3513.710817	763448.307036	41.530752
3513.557386	763221.728045	41.535757
3513.378838	762983.901932	41.540762
3513.668433	762748.901002	41.545767
3513.507421	762519.441586	41.550772
3512.986513	762285.102246	41.555776
3512.913348	762048.906183	41.560781
3513.150663	761821.283500	41.565786
3512.774838	761603.521675	41.570791
3512.703380	761371.595543	41.575796
3512.702892	761159.481139	41.580800
3512.533681	760937.226377	41.585805
3512.593003	760730.812489	41.590810
3512.552820	760497.867733	41.595815
3512.501204	760292.693516	41.600820
3511.979178	760082.262883	41.605824
3512.138608	759857.060704	41.610829
3511.996428	759652.624135	41.615834
3511.632919	759451.475011	41.620839
3512.007345	759247.929227	41.625844
3511.813745	759043.040615	41.630848
3511.570354	758835.884815	41.635853
3511.389988	758634.782550	41.640858
3511.214384	758428.097917	41.645863
3511.543803	758233.316197	41.650868
3511.147574	758038.649052	41.655872
3511.186014	757842.326065	41.660877
3510.997738	757649.292635	41.665882
3510.555250	757454.519459	41.670887
3510.671099	757259.106402	41.675892
3510.476785	757085.999090	41.680896
3510.565580	756905.783109	41.685901
3510.395990	756732.762418	41.690906
3510.588605	756548.374781	41.695911
3510.544918	756349.805701	41.700916
3510.398158	756187.578920	41.705920
3510.160147	756007.543667	41.710925
3510.180202	755830.917150	41.715930
3509.949737	755653.488619	41.720935
3510.125078	755484.825714	41.725940
3509.794386	755312.984209	41.730944
3510.056036	755139.905768	41.735949
3509.964963	754963.178796	41.740954
3509.504864	754799.344996	41.745959
3509.687945	754622.219393	41.750964
3509.433472	754473.008219	41.755968
3509.424284	754294.326787	41.760973
3509.653537	754137.030760	41.765978
3509.386923	753972.258654	41.770983
3509.281468	753804.592575	41.775988
3509.235091	753652.220385	41.780992
3508.928951	753483.345904	41.785997
3509.124397	753330.581839	41.791002
3509.059815	753174.450272	41.796007
3509.329625	753012.186408	41.801012
3508.875764	752860.458259	41.806016
3509.235253	752710.222788	41.811021
3508.655905	752548.484139	41.816026
3508.782897	752397.243781	41.821031
3508.956280	752259.623696	41.826036
3508.160225	752113.122858	41.831040
3508.204392	751953.837175	41.836045
3508.568020	751824.425968	41.841050
3508.459040	751670.592572	41.846055
3508.435727	751524.743490	41.851060
3508.003493	751398.370397	41.856064
3507.938839	751246.595744	41.861069
3508.152517	751116.160113	41.866074
3507.693571	750988.796829	41.871079
3508.271072	750837.995048	41.876084
3507.784467	750724.462920	41.881088
3508.025072	750570.204241	41.886093
3507.938943	750439.213820	41.891098
3507.665271	750309.635275	41.896103
3507.956057	750169.785046	41.901108
3507.846105	750048.770856	41.906112
3507.797894	749905.711228	41.911117
3507.709613	749783.207253	41.916122
3507.510425	749639.377138	41.921127
3507.352646	749514.756002	41.926132
3507.226512	749385.285905	41.931136
3507.333197	749260.567707	41.936141
3507.389439	749147.960562	41.941146
3507.133898	749023.891130	41.946151
3507.578702	748894.565820	41.951156
3507.339000	748778.494063	41.956160
3507.148944	748645.316456	41.961165
3506.762146	748530.105199	41.966170
3506.980731	748418.350132	41.971175
3507.125923	748292.424174	41.976180
3506.845789	748181.785545	41.981184
3506.992594	748053.088309	41.986189
3506.709385	747939.926631	41.991194
3506.966040	747834.481998	41.996199
3506.817932	747697.822181	42.001204
3506.980993	747590.857769	42.006208
3506.859086	747479.145329	42.011213
3506.683068	747376.286089	42.016218
3506.882920	747252.755820	42.021223
3506.933814	747140.417027	42.026228
3506.424919	747024.758833	42.031232
3506.538852	746910.281256	42.036237
3506.630859	746799.314575	42.041242
3506.442998	746701.341163	42.046247
3506.313495	746583.834708	42.051252
3506.053641	746479.692456	42.056256
3506.205017	746362.680061	42.061261
3505.758477	746265.188621	42.066266
3505.609767	746170.909006	42.071271
3506.135807	746070.635316	42.076276
3505.783724	745982.169844	42.081280
3505.806103	745879.406479	42.086285
3506.068006	745787.229408	42.091290
3505.715745	745691.198128	42.096295
3505.730595	745597.230653	42.101300
3505.524640	745503.496154	42.106304
3505.793469	745401.476792	42.111309
3506.167395	745303.788754	42.116314
3505.972068	745214.843897	42.121319
3506.045014	745115.126956	42.126324
3505.679656	745024.576677	42.131328
3505.851349	744921.182943	42.136333
3505.551765	744825.330102	42.141338
3505.592213	744743.509041	42.146343
3505.870134	744646.322985	42.151348
3505.696460	744552.324615	42.156352
3505.651251	744454.349009	42.161357
3505.911245	744365.714995	42.166362
3505.377010	744272.464803	42.171367
3505.201067	744176.682542	42.176372
3504.883162	744103.367839	42.181376
3505.616144	744009.164141	42.186381
3505.659989	743929.707142	42.191386
3505.252257	743847.208987	42.196391
3505.256811	743756.434804	42.201396
3505.215612	743674.912714	42.206400
3505.323268	743580.065289	42.211405
3505.430674	743496.044745	42.216410
3504.896683	743420.386019	42.221415
3504.809779	743335.308022	42.226420
3505.013328	743255.471793	42.231424
3505.279554	743170.778834	42.236429
3505.341506	743092.942083	42.241434
3504.993031	743009.139795	42.246439
3505.035892	742915.827868	42.251444
3505.066084	742841.059541	42.256448
3505.053736	742762.836196	42.261453
3505.199876	742669.751577	42.266458
3504.772952	742592.831053	42.271463
3504.926909	742522.835817	42.276468
3504.841294	742446.253218	42.281472
3505.061887	742375.850105	42.286477
3505.264949	742282.059235	42.291482
3504.717164	742206.737272	42.296487
3504.606562	742111.858690	42.301492
3504.558904	742032.941605	42.306496
3504.736185	741970.701590	42.311501
3504.639862	741882.592874	42.316506
3504.465760	741813.733370	42.321511
3504.560791	741735.729419	42.326516
3504.337019	741693.483176	42.331520
3504.425722	741612.660168	42.336525
3504.575537	741535.881584	42.341530
3504.454635	741476.851937	42.346535
3504.865969	741396.913220	42.351540
3504.747716	741321.462579	42.356544
3504.519979	741254.535842	42.361549
3504.769291	741177.836303	42.366554
3504.455844	741110.180606	42.371559
3504.598949	741035.079833	42.376564
3504.208440	740966.001310	42.381568
3504.101214	740890.495283	42.386573
3504.322272	740821.017974	42.391578
3504.206422	740764.455157	42.396583
3504.352377	740695.483721	42.401588
3504.373533	740640.282333	42.406592
3504.294271	740561.256850	42.411597
3504.566111	740482.420037	42.416602
3504.241607	740417.480632	42.421607
3504.805311	740351.207246	42.426612
3504.354578	740281.638050	42.431616
3503.739564	740209.918922	42.436621
3503.946044	740147.511374	42.441626
3504.095469	740088.624691	42.446631
3504.058398	740027.295074	42.451636
3504.297236	739969.728318	42.456640
3504.096628	739901.202797	42.461645
3504.382420	739834.525704	42.466650
3504.176581	739761.844720	42.471655
3504.623345	739686.334878	42.476660
3504.232133	739630.402940	42.481664
3504.184321	739562.492390	42.486669
3504.116306	739498.096803	42.491674
3504.032703	739442.953813	42.496679
3504.503159	739372.680711	42.501684
3504.254968	739299.854071	42.506688
3504.109029	739240.564547	42.511693
3504.236595	739181.823152	42.516698
3504.114995	739117.977482	42.521703
3504.304638	739062.143716	42.526708
3504.018849	738992.090799	42.531712
3504.356332	738918.916813	42.536717
3504.086151	738851.333654	42.541722
3504.085576	738798.695579	42.546727
3504.387254	738732.105571	42.551732
3504.097810	738664.326107	42.556736
3503.798807	738600.258146	42.561741
3504.018707	738536.450487	42.566746
3503.876906	738476.115632	42.571751
3503.985420	738421.428647	42.576756
3504.275338	738362.209184	42.581760
3503.954598	738290.918979	42.586765
3504.279199	738227.141068	42.591770
3504.004881	738166.479372	42.596775
3504.161474	738102.282860	42.601780
3504.284683	738046.551876	42.606784
3504.172591	737978.094148	42.611789
3504.033431	737918.002018	42.616794
3503.899515	737855.187279	42.621799
3503.914168	737794.821487	42.626804
3503.595624	737738.814789	42.631808
3503.754594	737681.788916	42.636813
3504.183661	737617.741527	42.641818
3503.499341	737567.137676	42.646823
3503.699124	737518.465995	42.651828
3504.072826	737469.418999	42.656832
3504.133187	737401.175308	42.661837
3504.040963	737341.466948	42.666842
3503.988899	737279.673297	42.671847
3503.981353	737215.397734	42.676852
3503.951490	737167.306055	42.681856
3503.802579	737106.318736	42.686861
3503.958753	737036.225282	42.691866
3503.858662	736977.010324	42.696871
3503.918527	736918.659280	42.701876
3503.626109	736860.613276	42.706880
3503.753013	736804.180234	42.711885
3503.867547	736758.981893	42.716890
3503.499440	736695.800741	42.721895
3503.410634	736639.402078	42.726900
3503.644798	736602.298767	42.731904
3503.786924	736549.572854	42.736909
3503.611229	736490.317262	42.741914
3503.072767	736445.620635	42.746919
3503.621774	736370.260508	42.751924
3503.706930	736326.153283	42.756928
3503.631576	736275.490385	42.761933
3503.861548	736219.927022	42.766938
3503.459713	736167.040777	42.771943
3503.822985	736092.005568	42.776948
3503.623963	736043.935007	42.781952
3503.724864	735997.843809	42.786957
3503.522701	735952.247690	42.791962
3503.391398	735902.779408	42.796967
3503.760038	735850.951887	42.801972
3503.418360	735801.270189	42.806977
3503.402790	735739.359645	42.811981
3503.587292	735690.332928	42.816986
3503.460666	735639.328014	42.821991
3503.495281	735593.443381	42.826996
3503.237294	735548.200603	42.832001
3503.095437	735490.565282	42.837005
3503.430869	735446.609949	42.842010
3503.346744	735393.567260	42.847015
3502.965665	735348.739584	42.852020
3503.244377	735301.922180	42.857025
3502.976605	735252.571358	42.862029
3503.554056	735208.871812	42.867034
3502.980949	735158.234371	42.872039
3503.371011	735118.673270	42.877044
3503.316037	735083.491383	42.882049
3503.148537	735029.123652	42.887053
3503.450428	734977.548970	42.892058
3503.106536	734927.961214	42.897063
3503.206951	734880.972751	42.902068
3502.937413	734842.459404	42.907073
3503.248021	734794.000396	42.912077
3503.514445	734748.171730	42.917082
3503.260164	734703.517544	42.922087
3503.069985	734655.437200	42.927092
3503.204903	734600.571258	42.932097
3503.326057	734560.358746	42.937101
3503.321842	734513.236878	42.942106
3503.004964	734471.363640	42.947111
3503.355082	734416.906478	42.952116
3503.182287	734383.621911	42.957121
3502.846607	734332.692639	42.962125
3503.319421	734291.480345	42.967130
3502.852706	734257.897185	42.972135
3503.170219	734206.809990	42.977140
3503.195342	734167.799352	42.982145
3503.251792	734123.437249	42.987149
3503.134563	734074.846401	42.992154
3502.868945	734024.844161	42.997159
3503.131006	733986.932145	43.002164
3503.133548	733947.528145	43.007169
3503.144813	733910.251117	43.012173
3503.379968	733851.403361	43.017178
3503.233403	733810.043146	43.022183
3503.656809	733760.767287	43.027188
3503.123043	733720.064447	43.032193
3503.115836	733668.334293	43.037197
3503.242768	733621.977659	43.042202
3503.102174	733579.080645	43.047207
3503.068904	733531.908314	43.052212
3502.858769	733495.457922	43.057217
3502.731817	733452.458975	43.062221
3503.147184	733415.360600	43.067226
3503.122808	733370.710637	43.072231
3503.230331	733327.969426	43.077236
3502.935278	733281.432835	43.082241
3503.052411	733243.392685	43.087245
3503.276319	733192.116458	43.092250
3502.925334	733150.340976	43.097255
3502.985057	733097.754512	43.102260
3502.654315	733068.401611	43.107265
3502.765675	733033.232860	43.112269
3502.814016	732993.321570	43.117274
3502.550021	732959.798601	43.122279
3502.918934	732911.467193	43.127284
3502.762199	732882.580029	43.132289
3502.798491	732834.154438	43.137293
3502.692840	732785.652925	43.142298
3502.392451	732768.423697	43.147303
3502.869776	732730.816878	43.152308
3502.825468	732693.840441	43.157313
3503.281142	732664.554532	43.162317
3503.147433	732613.185024	43.167322
3502.794996	732570.020484	43.172327
3502.802944	732528.628234	43.177332
3502.796738	732483.871348	43.182337
3503.006017	732448.881963	43.187341
3502.820786	732410.937223	43.192346
3502.309451	732373.145060	43.197351
3502.814803	732336.819099	43.202356
3502.571223	732304.032722	43.207361
3502.150703	732263.798982	43.212365
3502.724023	732243.651973	43.217370
3502.486297	732205.912970	43.222375
3502.847610	732168.768270	43.227380
3502.890048	732133.557446	43.232385
3502.806980	732095.891473	43.237389
3502.927634	732051.210315	43.242394
3502.490893	732013.354662	43.247399
3502.816979	731974.085771	43.252404
3502.666696	731939.995173	43.257409
3502.633666	731905.191905	43.262413
3503.147230	731865.891599	43.267418
3502.559110	731846.826243	43.272423
3502.807377	731790.635122	43.277428
3502.565908	731767.056074	43.282433
3502.774984	731734.985052	43.287437
3502.850552	731697.241568	43.292442
3502.505585	731668.876237	43.297447
3502.974020	731619.926524	43.302452
3502.855828	731583.897996	43.307457
3502.734133	731550.890413	43.312461
3502.489322	731517.358293	43.317466
3502.209011	731470.363177	43.322471
3502.441229	731440.119316	43.327476
3502.749760	731414.715504	43.332481
3502.423633	731378.373698	43.337485
3502.762078	731352.370547	43.342490
3502.715602	731322.271203	43.347495
3502.919480	731273.263952	43.352500
3502.855572	731238.561943	43.357505
3502.651080	731202.050747	43.362509
3502.913974	731158.628723	43.367514
3502.658190	731121.481865	43.372519
3502.549881	731082.230709	43.377524
3502.330310	731049.633367	43.382529
3502.633393	731035.420759	43.387533
3502.744948	730990.487650	43.392538
3502.517581	730957.296978	43.397543
3502.458208	730919.968272	43.402548
3502.454552	730904.320354	43.407553
3502.184100	730870.789780	43.412557
3502.802963	730837.459185	43.417562
3502.188655	730803.885949	43.422567
3502.515202	730769.464247	43.427572
3502.378224	730736.109210	43.432577
3502.335015	730713.138207	43.437581
3502.457401	730681.176346	43.442586
3502.278282	730652.582036	43.447591
3502.639144	730620.035896	43.452596
3502.473068	730594.856287	43.457601
3502.291860	730566.162971	43.462605
3502.652988	730526.683209	43.467610
3501.915056	730501.845151	43.472615
3502.815888	730462.424720	43.477620
3502.510092	730428.254334	43.482625
3502.430086	730398.355180	43.487629
3502.354299	730360.432317	43.492634
3502.640193	730340.922246	43.497639
3502.602265	730304.726233	43.502644
3502.897246	730273.081000	43.507649
3502.942330	730226.025052	43.512653
3502.857067	730197.562248	43.517658
3502.540722	730159.133305	43.522663
3502.795133	730119.421523	43.527668
3502.017485	730080.325330	43.532673
3502.354606	730061.549037	43.537677
3502.744729	730031.026283	43.542682
3502.456923	730006.162061	43.547687
3502.735928	729971.299078	43.552692
3502.446836	729938.262984	43.557697
3502.156336	729894.628225	43.562701
3502.458299	729877.541217	43.567706
3502.491189	729850.593069	43.572711
3502.226961	729805.021937	43.577716
3502.370003	729781.918556	43.582721
3502.394412	729753.782820	43.587725
3502.303555	729724.328723	43.592730
3502.301140	729694.067496	43.597735
3502.674005	729663.249039	43.602740
3502.482171	729630.740481	43.607745
3502.402854	729599.798174	43.612749
3502.518127	729565.554777	43.617754
3502.267683	729536.968288	43.622759
3502.705795	729513.716470	43.627764
3502.590231	729474.359676	43.632769
3502.631965	729439.236333	43.637773
3502.769077	729409.446355	43.642778
3502.466022	729380.917516	43.647783
3502.790851	729336.039179	43.652788
3502.762073	729310.139539	43.657793
3502.415251	729277.407453	43.662797
3502.476042	729239.853104	43.667802
3502.476013	729216.424976	43.672807
3502.486680	729170.260150	43.677812
3502.345619	729151.907272	43.682817
3502.969330	729117.429622	43.687821
3502.809445	729081.892172	43.692826
3502.576654	729053.003882	43.697831
3502.511048	729011.407674	43.702836
3502.547105	728979.007559	43.707841
3502.412700	728945.347551	43.712845
3502.762609	728918.294549	43.717850
3502.229425	728876.725162	43.722855
3502.796124	728834.280868	43.727860
3502.652636	728813.401423	43.732865
3502.637280	728777.937900	43.737869
3502.707538	728749.543471	43.742874
3502.706702	728717.544667	43.747879
3502.534040	728667.741675	43.752884
3502.653019	728652.366424	43.757889
3502.636285	728611.156396	43.762893
3502.534004	728573.873522	43.767898
3502.335048	728550.525791	43.772903
3502.316783	728512.287623	43.777908
3502.310853	728488.660234	43.782913
3502.313141	728453.885891	43.787917
3502.721251	728427.118887	43.792922
3502.595191	728401.380995	43.797927
3502.271990	728371.712608	43.802932
3502.840702	728333.723642	43.807937
3502.486772	728302.623509	43.812941
3502.578578	728263.127621	43.817946
3502.324161	728241.868693	43.822951
3502.211300	728202.009936	43.827956
3502.407747	728183.846952	43.832961
3502.407364	728150.508340	43.837965
3502.430735	728119.048113	43.842970
3502.041654	728095.829482	43.847975
3502.051401	728060.854084	43.852980
3501.914442	728037.593745	43.857985
3502.337001	728012.110996	43.862989
3502.275490	727980.961454	43.867994
3502.216055	727962.988756	43.872999
3502.537588	727927.020178	43.878004
3502.283203	727894.614073	43.883009
3502.756463	727868.379437	43.888013
3502.459302	727827.657512	43.893018
3502.429687	727805.964091	43.898023
3502.404727	727778.523227	43.903028
3502.554696	727758.633063	43.908033
3502.229867	727713.803313	43.913037
3502.540615	727682.095892	43.918042
3502.139997	727665.912671	43.923047
3502.180410	727623.647891	43.928052
3502.660053	727606.675483	43.933057
3502.054051	727569.669181	43.938061
3502.146928	727556.624600	43.943066
3502.119672	727515.361234	43.948071
3502.225096	727493.099775	43.953076
3502.479957	727465.760380	43.958081
3502.142586	727445.157085	43.963085
3502.443993	727410.626267	43.968090
3502.060532	727398.155340	43.973095
3502.464319	727360.634913	43.978100
3502.434001	727343.597360	43.983105
3502.284517	727302.749400	43.988109
3502.349488	727275.837000	43.993114
3502.462512	727243.367774	43.998119
3502.311633	727200.389180	44.003124
3502.275372	727184.194510	44.008129
3502.620468	727159.861375	44.013133
3502.617026	727119.731591	44.018138
3502.150135	727086.762769	44.023143
3502.247613	727058.258890	44.028148
3502.363043	727035.201831	44.033153
3502.166779	727008.430685	44.038157
3502.365646	726981.049354	44.043162
3502.502265	726952.984562	44.048167
3502.574634	726926.614789	44.053172
3502.452134	726885.363938	44.058177
3502.190683	726863.012581	44.063181
3502.503704	726814.802806	44.068186
3502.072242	726797.037480	44.073191
3502.228630	726771.991101	44.078196
3502.464007	726750.994407	44.083201
3501.958803	726733.637462	44.088205
3502.368993	726692.941971	44.093210
3502.193659	726682.120232	44.098215
3502.573892	726646.334544	44.103220
3502.308603	726622.942683	44.108225
3502.260773	726593.916116	44.113229
3502.516245	726558.794714	44.118234
3502.249100	726526.137549	44.123239
3502.542872	726494.031950	44.128244
3502.336156	726466.121157	44.133249
3502.329081	726441.943016	44.138253
3502.431470	726402.733691	44.143258
3501.932824	726379.032746	44.148263
3502.259907	726346.078759	44.153268
3502.219218	726320.270697	44.158273
3502.278522	726299.004567	44.163277
3502.460373	726266.718325	44.168282
3501.861527	726248.582994	44.173287
3502.231060	726215.621489	44.178292
3502.574011	726194.209253	44.183297
3502.284304	726163.090389	44.188301
3502.394023	726133.342537	44.193306
3502.445097	726103.653790	44.198311
3502.616593	726064.530563	44.203316
3502.299882	726042.334720	44.208321
3502.103918	726011.843989	44.213325
3502.557739	725980.453270	44.218330
3502.260697	725957.510695	44.223335
3502.462762	725922.345820	44.228340
3502.468030	725891.871038	44.233345
3502.265173	725870.845199	44.238349
3502.534772	725839.781605	44.243354
3502.525380	725815.849759	44.248359
3502.688840	725791.839809	44.253364
3502.586183	725755.782945	44.258369
3502.402045	725720.433080	44.263373
3502.488509	725692.620002	44.268378
3502.189046	725658.329472	44.273383
3502.639544	725626.095554	44.278388
3502.869700	725592.113905	44.283393
3502.462126	725559.376920	44.288397
3502.678880	725522.523103	44.293402
3502.381214	725492.691396	44.298407
3502.358862	725461.624924	44.303412
3502.308740	725429.869154	44.308417
3502.270080	725397.070735	44.313421
3502.504499	725369.033967	44.318426
3502.231257	725338.107476	44.323431
3502.294173	725312.675612	44.328436
3502.349916	725284.073337	44.333441
3502.215608	725265.611507	44.338445
3502.199482	725222.501229	44.343450
3502.460995	725204.667816	44.348455
3502.154369	725171.763984	44.353460
3501.988760	725150.779718	44.358465
3502.310784	725122.876344	44.363469
3502.686296	725100.117889	44.368474
3502.560313	725082.100279	44.373479
3502.437091	725039.006685	44.378484
3502.343546	725007.752003	44.383489
3502.105664	724977.115666	44.388493
3502.489922	724946.327147	44.393498
3502.254602	724924.213979	44.398503
3502.110001	724892.620373	44.403508
3502.598985	724867.364716	44.408513
3502.332866	724843.274108	44.413517
3502.115389	724808.817848	44.418522
3502.164395	724790.423861	44.423527
3502.488502	724752.508193	44.428532
3502.417260	724724.024011	44.433537
3502.466032	724699.781982	44.438541
3502.371284	724659.903007	44.443546
3502.224765	724638.071789	44.448551
3502.271529	724606.098640	44.453556
3502.412112	724590.960010	44.458561
3502.139754	724560.327800	44.463565
3502.424049	724522.665431	44.468570
3501.876935	724501.891047	44.473575
3502.014512	724478.575367	44.478580
3502.200782	724445.141373	44.483585
3502.146794	724420.221613	44.488589
3502.590546	724380.252556	44.493594
3502.308403	724377.176781	44.498599
3502.512566	724333.282142	44.503604
3502.218120	724310.978824	44.508609
3502.506411	724284.564995	44.513613
3502.812797	724251.952962	44.518618
3502.333475	724227.053139	44.523623
3502.295864	724192.663785	44.528628
3502.639908	724165.348281	44.533633
3502.178561	724137.372402	44.538637
3502.141112	724104.370384	44.543642
3502.195668	724081.810691	44.548647
3502.366994	724056.654458	44.553652
3502.242864	724032.240705	44.558657
3502.171718	724006.876460	44.563661
3502.411864	723975.711566	44.568666
3502.126815	723943.740956	44.573671
3502.158287	723912.411954	44.578676
3502.042513	723884.477401	44.583681
3501.999035	723878.239623	44.588685
3502.518490	723836.520742	44.593690
3502.191777	723822.300280	44.598695
3502.436572	723782.460239	44.603700
3502.435808	723759.165320	44.608705
3502.250241	723728.267893	44.613709
3502.319219	723703.771784	44.618714
3502.385383	723659.053702	44.623719
3502.099390	723640.266265	44.628724
3502.365522	723612.168734	44.633729
3502.541920	723598.261507	44.638733
3502.477944	723558.768653	44.643738
3502.432378	723537.413536	44.648743
3502.218911	723500.472870	44.653748
3502.692287	723462.625814	44.658753
3502.196129	723441.691654	44.663757
3502.338813	723409.004135	44.668762
3502.169295	723399.168430	44.673767
3502.303771	723362.268947	44.678772
3502.257901	723338.435042	44.683777
3501.663504	723312.262678	44.688781
3502.387883	723285.525968	44.693786
3502.236555	723263.146663	44.698791
3502.148294	723244.127474	44.703796
3501.972039	723204.998397	44.708801
3502.012357	723199.440242	44.713805
3502.056400	723159.184167	44.718810
3501.878092	723141.121363	44.723815
3502.106692	723106.881891	44.728820
3502.096394	723103.909547	44.733825
3502.123679	723075.006889	44.738829
3502.257242	723037.858268	44.743834
3502.016558	723017.674030	44.748839
3502.282265	722994.134773	44.753844
3502.294752	722971.331135	44.758849
3502.263731	722929.896660	44.763853
3502.462301	722909.491075	44.768858
3502.129763	722888.429410	44.773863
3502.198564	722855.057905	44.778868
3502.581617	722824.459958	44.783873
3502.070665	722798.520061	44.788877
3502.291696	722774.442272	44.793882
3502.374122	722748.503587	44.798887
3502.118377	722721.430853	44.803892
3502.466988	722679.684721	44.808897
3502.536938	722665.793468	44.813901
3502.540651	722632.778786	44.818906
3502.079834	722607.920586	44.823911
3502.297138	722578.390032	44.828916
3502.348489	722552.852423	44.833921
3502.173470	722531.763893	44.838925
3502.326537	722505.217949	44.843930
3502.415810	722481.309733	44.848935
3502.422807	722444.625449	44.853940
3502.269649	722415.551932	44.858945
3502.155474	722386.174454	44.863949
3502.315128	722356.503892	44.868954
3501.959409	722336.287370	44.873959
3502.540487	722308.926684	44.878964
3502.452475	722276.470994	44.883969
3502.229251	722253.010193	44.888973
3502.532472	722208.542646	44.893978
3502.375857	722199.397411	44.898983
3502.074619	722159.639525	44.903988
3502.266370	722132.590276	44.908993
3502.442900	722101.180935	44.913997
3502.551708	722070.526247	44.919002
3502.373194	722055.385980	44.924007
3502.220130	722012.132770	44.929012
3502.234750	721996.216954	44.934017
3502.329418	721963.482064	44.939021
3502.523107	721924.682572	44.944026
3502.367755	721900.565113	44.949031
3502.010413	721870.730121	44.954036
3502.291532	721838.856374	44.959041
3501.899614	721822.561030	44.964045
3502.341053	721781.191685	44.969050
3502.100583	721772.109370	44.974055
3502.001330	721752.444073	44.979060
3502.135964	721725.749942	44.984065
3501.812918	721699.775630	44.989069
3502.184395	721681.817354	44.994074
3501.776375	721653.031034	44.999079
3502.468911	721637.647328	45.004084
3502.370661	721601.769882	45.009089
3502.193506	721578.696195	45.014093
3502.340362	721540.993323	45.019098
3502.133545	721524.666891	45.024103
3502.021640	721498.706737	45.029108
3502.353859	721468.409633	45.034113
3501.833946	721456.051300	45.039117
3502.286157	721412.397762	45.044122
3502.137914	721399.383167	45.049127
3502.135302	721366.810686	45.054132
3502.068289	721341.388004	45.059137
3501.934336	721322.718976	45.064141
3502.047309	721305.992372	45.069146
3502.032994	721275.156716	45.074151
3502.222198	721248.699955	45.079156
3502.608891	721217.153482	45.084161
3502.020362	721205.599348	45.089165
3502.508216	721160.500813	45.094170
3502.339439	721142.035435	45.099175
3501.816172	721111.580510	45.104180
3502.228255	721091.184853	45.109185
3502.132198	721053.618953	45.114189
3501.967209	721030.392994	45.119194
3501.538710	721004.235555	45.124199
3502.000856	720988.293648	45.129204
3502.292729	720965.587198	45.134209
3502.116331	720943.651977	45.139213
3502.349274	720920.459306	45.144218
3502.408259	720891.841297	45.149223
3502.063717	720875.585861	45.154228
3502.555368	720849.871299	45.159233
3502.130010	720818.952932	45.164237
3502.242721	720783.037187	45.169242
3502.071430	720769.033762	45.174247
3502.338563	720737.455588	45.179252
3502.277683	720704.047212	45.184257
3501.973687	720682.181907	45.189261
3502.217631	720656.358814	45.194266
3502.273584	720633.640750	45.199271
3502.149876	720607.283089	45.204276
3502.236045	720578.609941	45.209281
3502.075166	720558.951969	45.214285
3502.242425	720524.612783	45.219290
3501.949229	720515.438608	45.224295
3502.071790	720477.982834	45.229300
3502.041807	720462.071427	45.234305
3502.009955	720438.871460	45.239309
3502.191280	720403.785699	45.244314
3502.110089	720389.072609	45.249319
3502.054589	720368.405138	45.254324
3502.254149	720339.315807	45.259329
3502.131361	720317.766775	45.264333
3502.405454	720291.640076	45.269338
3502.217086	720259.440956	45.274343
3502.560536	720230.079609	45.279348
3502.940257	720202.893939	45.284353
3502.521355	720178.517387	45.289357
3502.590706	720144.639036	45.294362
3502.200642	720115.745247	45.299367
3501.923757	720083.163342	45.304372
3502.257528	720059.654144	45.309377
3501.935818	720038.186750	45.314381
3502.181167	720007.948232	45.319386
3502.021519	719994.586207	45.324391
3502.046395	719969.987161	45.329396
3502.397297	719935.863223	45.334401
3502.221605	719914.817734	45.339405
3502.135734	719891.525967	45.344410
3502.133718	719852.501116	45.349415
3501.864472	719844.909050	45.354420
3502.250280	719816.332668	45.359425
3502.198384	719796.406997	45.364429
3502.411843	719758.337957	45.369434
3502.086329	719743.614394	45.374439
3502.113234	719704.187378	45.379444
3502.296075	719689.330369	45.384449
3502.272121	719653.184326	45.389453
3502.211325	719629.441398	45.394458
3502.006929	719600.961526	45.399463
3502.124149	719576.494870	45.404468
3502.295676	719548.746305	45.409473
3502.279744	719530.152981	45.414477
3502.217989	719498.723484	45.419482
3502.150595	719476.816021	45.424487
3502.127111	719453.016852	45.429492
3502.062591	719419.901460	45.434497
3502.448582	719399.208429	45.439501
3502.606152	719365.510736	45.444506
3502.366793	719342.341905	45.449511
3502.336000	719304.806945	45.454516
3502.264562	719276.948737	45.459521
3502.100374	719265.569924	45.464525
3502.406629	719230.210684	45.469530
3502.117056	719208.041576	45.474535
3502.288859	719171.712418	45.479540
3502.132156	719159.439579	45.484545
3502.095250	719134.104373	45.489549
3502.317462	719102.031492	45.494554
3502.328082	719079.118291	45.499559
3502.363756	719037.504629	45.504564
3502.213375	719020.221721	45.509569
3502.431946	718994.645627	45.514573
3502.266941	718964.917277	45.519578
3501.811264	718932.608292	45.524583
3502.439810	718906.766006	45.529588
3502.389360	718883.019248	45.534593
3502.153194	718860.890009	45.539597
3502.333570	718828.872566	45.544602
3502.478711	718809.110444	45.549607
3502.014420	718773.529081	45.554612
3501.977091	718755.036743	45.559617
3502.278055	718728.999915	45.564621
3502.398743	718704.827698	45.569626
3501.988815	718664.575050	45.574631
3502.222624	718647.575228	45.579636
3502.214712	718610.628512	45.584641
3501.814759	718593.782601	45.589645
3502.116997	718563.529479	45.594650
3502.083175	718534.174741	45.599655
3501.959000	718520.606124	45.604660
3502.262037	718488.815145	45.609665
3501.863914	718478.664094	45.614669
3502.014199	718437.722898	45.619674
3501.951449	718423.796832	45.624679
3501.932139	718415.219953	45.629684
3502.412017	718396.889582	45.634689
3502.056004	718371.902219	45.639693
3502.088027	718339.411384	45.644698
3502.243317	718326.143579	45.649703
3502.245549	718295.046182	45.654708
3502.118088	718271.111986	45.659713
3502.268021	718237.559794	45.664717
3502.012501	718219.945372	45.669722
3501.946409	718194.760917	45.674727
3502.182667	718167.195489	45.679732
3502.218138	718138.621503	45.684737
3501.794440	718124.456826	45.689741
3501.848680	718090.622225	45.694746
3502.033152	718076.555650	45.699751
3501.939019	718045.869988	45.704756
3502.374009	718025.363883	45.709761
3502.087098	718020.054579	45.714765
3502.014077	717988.720451	45.719770
3502.238385	717965.223404	45.724775
3502.347590	717925.476838	45.729780
3502.405578	717899.675863	45.734785
3501.879343	717875.359849	45.739789
3502.267103	717848.066003	45.744794
3502.114108	717819.075585	45.749799
3501.975105	717798.266706	45.754804
3502.319073	717773.013416	45.759809
3502.092015	717763.527703	45.764813
3502.148532	717706.329616	45.769818
3502.135077	717628.161621	45.774823
3502.103467	717495.236086	45.779828
3501.953583	717300.920159	45.784833
3501.595626	717055.591615	45.789837
3501.799726	716743.443641	45.794842
3501.384497	716386.739039	45.799847
3501.257198	715967.562116	45.804852
3501.382016	715486.306364	45.809857
3500.637190	714962.397184	45.814861
3500.068553	714364.145734	45.819866
3499.890238	713717.702340	45.824871
3499.653652	713011.020768	45.829876
3499.135611	712248.639350	45.834881
3498.438312	711445.467093	45.839885
3498.304913	710560.911866	45.844890
3497.135988	709627.532720	45.849895
3496.405126	708643.482111	45.854900
3496.110897	707580.884190	45.859905
3495.144221	706472.672419	45.864909
3494.699248	705301.297043	45.869914
3494.039009	704079.075471	45.874919
3493.250975	702790.668685	45.879924
3492.297696	701443.210044	45.884929
3491.348516	700047.132207	45.889933
3490.784420	698586.939534	45.894938
3489.586183	697070.823457	45.899943
3488.416179	695487.159667	45.904948
3487.899654	693855.406617	45.909953
3486.478724	692171.865823	45.914957
3485.052231	690429.892801	45.919962
3483.914144	688627.316360	45.924967
3482.570456	686780.211355	45.929972
3481.631031	684878.096091	45.934977
3480.107719	682929.865316	45.939981
3479.062674	680909.465842	45.944986
3477.329066	678850.473972	45.949991
3475.977371	676731.162837	45.954996
3475.050321	674568.682686	45.960001
3473.045333	672353.532438	45.965005
3471.727493	670091.071772	45.970010
3470.313927	667782.147305	45.975015
3468.296474	665417.732262	45.980020
3467.000172	662996.872214	45.985025
3464.863997	660543.945518	45.990029
3463.527712	658033.048102	45.995034
3461.957549	655497.072288	46.000039
3459.932150	652888.332558	46.005044
3458.270585	650247.915515	46.010049
3456.289133	647560.719453	46.015053
3454.670170	644827.549762	46.020058
3452.195604	642052.726524	46.025063
3450.096556	639235.368515	46.030068
3448.011876	636376.457353	46.035073
3445.560497	633487.289441	46.040077
3444.165825	630555.095760	46.045082
3442.128068	627586.938427	46.050087
3439.239109	624583.379896	46.055092
3437.520192	621528.130866	46.060097
3435.445153	618442.959212	46.065101
3432.990701	615301.530566	46.070106
3430.495281	612153.498044	46.075111
3428.162061	608949.068840	46.080116
3426.224833	605716.967599	46.085121
3423.059065	602451.525096	46.090125
3420.951034	599137.634885	46.095130
3418.354624	595803.192276	46.100135
3415.896525	592430.604589	46.105140
3413.470488	589017.756734	46.110145
3410.735197	585594.186530	46.115149
3408.053057	582126.803125	46.120154
3405.173608	578630.458255	46.125159
3402.513034	575103.712077	46.130164
3400.156817	571557.909323	46.135169
3397.157833	567978.453982	46.140173
3394.564370	564353.526671	46.145178
3391.722246	560718.464350	46.150183
3388.642222	557061.229607	46.155188
3386.183956	553365.096921	46.160193
3382.836587	549645.771181	46.165197
3380.574682	545901.308255	46.170202
3377.185553	542128.990208	46.175207
3374.417602	538336.844080	46.180212
3371.447064	534518.646528	46.185217
3368.031570	530675.188630	46.190221
3365.384549	526798.945061	46.195226
3362.232072	522915.768856	46.200231
3358.772454	519006.594565	46.205236
3355.689327	515075.902969	46.210241
3352.732884	511132.477797	46.215245
3349.639586	507162.265761	46.220250
3346.148461	503180.626562	46.225255
3342.797482	499179.893506	46.230260
3339.772490	495149.011087	46.235265
3336.263997	491110.421904	46.240269
3333.124295	487055.039167	46.245274
3329.714188	482974.520103	46.250279
3326.155716	478883.123285	46.255284
3322.898462	474778.202061	46.260289
3319.190522	470669.766944	46.265293
3315.909058	466528.606589	46.270298
3312.313883	462393.303736	46.275303
3308.975170	458242.345532	46.280308
3306.083941	454080.018353	46.285313
3302.376293	449897.363968	46.290317
3298.711344	445696.275828	46.295322
3295.079189	441492.083216	46.300327
3291.356192	437270.921689	46.305332
3287.962495	433049.122485	46.310337
3284.291430	428823.860516	46.315341
3280.863879	424579.837803	46.320346
3277.023490	420320.522957	46.325351
3273.249241	416066.389679	46.330356
3269.591439	411804.398667	46.335361
3265.550620	407546.026579	46.340365
3261.965324	403268.319080	46.345370
3258.426302	398994.423552	46.350375
3254.324954	394713.331825	46.355380
3250.928113	390426.909995	46.360385
3246.989447	386136.143477	46.365389
3243.347176	381838.573226	46.370394
3239.641193	377543.580871	46.375399
3235.669092	373254.678547	46.380404
3231.694897	368951.881839	46.385409
3227.663098	364640.988006	46.390413
3224.020476	360338.779023	46.395418
3220.145843	356036.450939	46.400423
3216.410772	351736.760657	46.405428
3212.559473	347433.460767	46.410433
3208.222085	343131.389252	46.415437
3204.714546	338826.888152	46.420442
3200.545702	334525.745060	46.425447
3196.292491	330222.922062	46.430452
3192.759467	325923.854699	46.435457
3188.749320	321637.263001	46.440461
3184.437651	317341.119211	46.445466
3180.682898	313053.680797	46.450471
3176.667007	308773.295856	46.455476
3172.412449	304496.390975	46.460481
3168.310327	300232.673633	46.465485
3164.521559	295964.644411	46.470490
3160.700271	291709.287493	46.475495
3156.574094	287463.892298	46.480500
3152.643647	283211.919231	46.485505
3148.372692	278964.858703	46.490509
3144.143302	274726.792522	46.495514
3140.273560	270496.668660	46.500519
3136.078908	266283.660022	46.505524
3132.081296	262060.091783	46.510529
3127.690760	257871.336587	46.515533
3123.918566	253675.554356	46.520538
3119.771731	249485.431742	46.525543
3115.545058	245315.963971	46.530548
3111.446066	241139.323502	46.535553
3106.971284	236992.945907	46.540557
3103.207194	232857.542530	46.545562
3098.927227	228713.392623	46.550567
3094.640307	224601.301295	46.555572
3090.789880	220477.080587	46.560577
3086.533413	216381.704751	46.565581
3082.226226	212235.255338	46.570586
3078.098139	208125.468031	46.575591
3074.007852	204062.345042	46.580596
3069.815677	200004.371657	46.585601
3065.337591	195976.757153	46.590605
3061.345600	191949.832121	46.595610
3056.870658	187938.865778	46.600615
3052.718227	183934.168364	46.605620
3048.855166	179960.050967	46.610625
3044.348527	175995.478586	46.615629
3040.077250	172028.398394	46.620634
3035.911502	168093.920786	46.625639
3031.539986	164179.815964	46.630644
3027.710386	160262.376003	46.635649
3023.432777	156375.902092	46.640653
3019.180503	152491.874643	46.645658
3014.704814	148633.388691	46.650663
3010.491011	144778.426196	46.655668
3006.302550	140939.535761	46.660673
3001.930492	137140.467070	46.665677
2997.820190	133334.336895	46.670682
2993.226950	129559.307314	46.675687
2988.983274	125801.774309	46.680692
2985.021517	122058.401733	46.685697
2980.630173	118331.474354	46.690701
2976.516192	114613.083298	46.695706
2971.986437	110929.743477	46.700711
2967.671590	107254.517539	46.705716
2963.159222	103603.899576	46.710721
2958.665442	99970.327878	46.715725
2954.139164	96353.879222	46.720730
2949.970367	92774.254279	46.725735
2945.563676	89208.147395	46.730740
2941.311444	85653.133104	46.735745
2936.637216	82133.675642	46.740749
2932.536035	78631.626605	46.745754
2927.895905	75160.792403	46.750759
2923.171022	71700.039487	46.755764
2918.796109	68268.033210	46.760769
2914.403369	64869.393962	46.765773
2909.679581	61493.996715	46.770778
2905.151104	58145.199774	46.775783
2900.468291	54836.575552	46.780788
2895.616153	51531.754352	46.785793
2890.610121	48286.287224	46.790797
2885.760648	45056.303581	46.795802
2880.562865	41883.814014	46.800807
2874.316154	38755.912673	46.805812
2867.437445	35705.334796	46.810817
2856.978664	32805.982501	46.815821
2846.414370	30012.033546	46.820826
2836.168487	27333.788570	46.825831
2825.773768	24790.986637	46.830836
2816.562464	22378.941979	46.835841
2807.351992	20102.541676	46.840845
2798.428105	17957.168525	46.845850
2789.765367	15962.448812	46.850855
2781.967109	14081.087553	46.855860
2773.827185	12320.408527	46.860865
2765.810706	10721.031941	46.865869
2758.025854	9226.062368	46.870874
2749.190453	7878.127372	46.875879
2740.461198	6655.108101	46.880884
2731.887902	5575.804034	46.885889
2723.077754	4620.311655	46.890893
2714.790224	3771.676473	46.895898
2707.412434	3048.943691	46.900903
2700.615888	2432.090043	46.905908
2694.562983	1885.678987	46.910913
2688.658306	1443.212232	46.915917
2683.521894	1058.345838	46.920922
2679.138678	732.970586	46.925927
2674.272014	477.655260	46.930932
2670.519947	255.126843	46.935937
2662.729102	186.764990	46.940941
2653.446547	216.523211	46.945946
2648.846120	215.054425	46.950951
2646.561618	210.131076	46.955956
2646.544333	206.930734	46.960961
2645.402902	211.609420	46.965965
2644.159331	211.936825	46.970970
2642.288478	200.617692	46.975975
2639.362880	213.206568	46.980980
2637.515928	200.357458	46.985985
2634.104181	210.828186	46.990989
2630.971359	207.451480	46.995994
2627.396902	202.995386	47.000999
2624.512907	199.257143	47.006004
2621.622485	199.487888	47.011009
2618.335685	202.869267	47.016013
2615.382909	197.786060	47.021018
2612.134276	188.240481	47.026023
2608.408718	201.412495	47.031028
2605.715096	194.210507	47.036033
2602.586118	204.764435	47.041037
2599.048737	200.454788	47.046042
2596.197183	196.597148	47.051047
2592.457110	194.228253	47.056052
2589.281788	194.701400	47.061057
2585.771115	191.791040	47.066061
2582.433445	195.964276	47.071066
2579.389998	187.629683	47.076071
2575.668052	194.519383	47.081076
2572.410023	190.438158	47.086081
2568.767218	190.089583	47.091085
2565.797478	193.408209	47.096090
2562.610330	190.113140	47.101095
2559.170644	190.344384	47.106100
2555.879301	179.319535	47.111105
2552.274744	185.345653	47.116109
2549.081965	183.718061	47.121114
2545.506225	187.353586	47.126119
2541.923374	192.711489	47.131124
2538.548395	183.858172	47.136129
2535.456133	186.637969	47.141133
2532.250100	192.235619	47.146138
2528.650939	180.154910	47.151143
2525.196927	192.739663	47.156148
2521.851760	190.528641	47.161153
2518.472659	189.356298	47.166157
2514.836753	181.911264	47.171162
2510.758989	175.137497	47.176167
2506.955671	177.112497	47.181172
2504.870176	172.634345	47.186177
2500.916185	174.989626	47.191181
2496.828106	172.313563	47.196186
2493.556092	175.929777	47.201191
2490.289426	185.135752	47.206196
2487.351157	174.547219	47.211201
2484.020574	175.715436	47.216205
2480.625807	176.789263	47.221210
2477.108576	181.366947	47.226215
2473.547521	178.988925	47.231220
2470.524003	178.427106	47.236225
2466.546727	174.556634	47.241229
2462.880692	167.797049	47.246234
2459.234585	165.610093	47.251239
2455.569502	173.009878	47.256244
2452.900329	170.206611	47.261249
2449.238735	179.713612	47.266253
2445.896139	173.460505	47.271258
2442.528825	167.988805	47.276263
2438.654604	178.100825	47.281268
2435.576742	165.344708	47.286273
2432.015501	174.965200	47.291277
2428.292863	167.703087	47.296282
2425.047911	170.738446	47.301287
2421.277429	172.215530	47.306292
2417.949141	168.599108	47.311297
2414.214580	164.928584	47.316301
2410.841694	169.649234	47.321306
2407.636062	164.972003	47.326311
2404.084592	167.711047	47.331316
2400.397497	169.123271	47.336321
2396.908077	173.983544	47.341325
2393.212423	167.449137	47.346330
2390.310153	164.439683	47.351335
2386.479021	169.985091	47.356340
2382.999864	168.024808	47.361345
2379.400920	168.119265	47.366349
2376.114422	162.449960	47.371354
2372.853078	164.164107	47.376359
2369.212072	175.509725	47.381364
2365.958711	165.068218	47.386369
2362.228774	159.843715	47.391373
2358.915247	160.051510	47.396378
2355.052432	161.395682	47.401383
2351.633254	168.503530	47.406388
2348.314673	160.386218	47.411393
2344.740132	167.650158	47.416397
2341.272996	175.679219	47.421402
2338.414843	166.688454	47.426407
2334.280755	174.655539	47.431412
2331.256262	166.908048	47.436417
2327.396159	162.093227	47.441421
2323.841617	172.998937	47.446426
2320.619237	177.664607	47.451431
2316.844183	173.142219	47.456436
2313.556003	162.702754	47.461441
2309.836601	169.233046	47.466445
2306.204411	168.747342	47.471450
2302.668815	157.461693	47.476455
2299.467473	163.006400	47.481460
2296.392501	162.768927	47.486465
2292.765798	158.492427	47.491469
2289.114667	167.225016	47.496474
2285.677636	170.154233	47.501479
2281.815956	169.962580	47.506484
2278.349755	160.175534	47.511489
2274.935291	168.812227	47.516493
2271.481822	158.048822	47.521498
2268.343435	163.664655	47.526503
2264.388576	167.349935	47.531508
2261.361657	165.841974	47.536513
2257.344022	166.539250	47.541517
2253.797222	168.415452	47.546522
2250.690974	163.804214	47.551527
2246.929771	162.762045	47.556532
2243.779946	158.262992	47.561537
2240.240756	173.709755	47.566541
2236.882679	164.575250	47.571546
2233.235212	161.117038	47.576551
2229.724953	164.048909	47.581556
2225.957814	159.052271	47.586561
2222.515956	163.372185	47.591565
2219.089785	155.624791	47.596570
2216.023571	159.045575	47.601575
2211.970419	164.127707	47.606580
2208.620667	156.817242	47.611585
2205.403833	157.218749	47.616589
2201.441528	159.245881	47.621594
2198.606947	153.528143	47.626599
2194.816356	154.453404	47.631604
2191.333594	157.938046	47.636609
2187.512088	157.651822	47.641613
2183.987859	151.478245	47.646618
2180.719623	160.179847	47.651623
2177.158168	162.937668	47.656628
2173.576160	156.755679	47.661633
2170.305969	165.945632	47.666637
2166.634122	151.395128	47.671642
2163.352475	155.245600	47.676647
2159.362972	154.965431	47.681652
2156.264145	153.017110	47.686657
2152.896128	155.864371	47.691661
2149.123331	159.534674	47.696666
2146.167932	152.342669	47.701671
2142.618543	153.505799	47.706676
2139.121505	149.300171	47.711681
2135.435854	155.669896	47.716685
2131.961500	151.777453	47.721690
2128.230529	158.964152	47.726695
2124.341051	159.516447	47.731700
2121.390858	158.979641	47.736705
2117.836879	157.304827	47.741709
2114.090394	160.379979	47.746714
2110.984400	151.076475	47.751719
2107.297669	154.513945	47.756724
2103.732150	146.202376	47.761729
2100.206380	158.797418	47.766733
2096.511730	155.280011	47.771738
2093.242335	151.010777	47.776743
2089.980362	159.990434	47.781748
2086.823878	139.546838	47.786753
2082.626994	153.512122	47.791757
2079.141720	153.240320	47.796762
2075.873272	145.090476	47.801767
2072.503787	157.744186	47.806772
2069.220852	140.247428	47.811777
2065.343916	151.348011	47.816781
2061.653053	159.733478	47.821786
2058.224254	147.013516	47.826791
2054.356222	160.445580	47.831796
2051.405484	144.282055	47.836801
2047.660861	154.365822	47.841805
2043.948203	149.826653	47.846810
2040.927816	148.384259	47.851815
2037.262233	155.540883	47.856820
2034.331363	143.078336	47.861825
2030.752255	155.630324	47.866829
2026.787755	148.427641	47.871834
2023.402067	143.214457	47.876839
2019.438320	150.460784	47.881844
2016.507167	144.571447	47.886849
2013.013236	151.829192	47.891853
2009.438875	146.584027	47.896858
2006.031451	141.866016	47.901863
2001.910994	147.496578	47.906868
1998.671382	140.925478	47.911873
1995.204975	147.884653	47.916877
1991.574833	151.890075	47.921882
1988.243854	140.671162	47.926887
1984.692753	145.315343	47.931892
1981.309711	143.159512	47.936897
1978.255578	151.247863	47.941901
1974.770190	150.372102	47.946906
1971.225373	149.219426	47.951911
1967.495110	149.736868	47.956916
1963.954591	147.472868	47.961921
1960.281159	149.733689	47.966925
1956.652394	152.329321	47.971930
1953.307094	139.802277	47.976935
1949.673990	148.986770	47.981940
1946.349925	144.312067	47.986945
1942.725197	154.449709	47.991949
1939.274243	145.865973	47.996954
1936.125206	146.601014	48.001959
1932.166748	151.801714	48.006964
1928.919320	139.682014	48.011969
1925.477201	151.484444	48.016973
1921.842510	148.189741	48.021978
1918.800726	143.346481	48.026983
1914.694949	151.033321	48.031988
1911.238014	137.987598	48.036993
1907.481561	144.218998	48.041997
1904.015939	146.357129	48.047002
1900.891393	140.662224	48.052007
1897.479454	143.859881	48.057012
1893.919170	133.420522	48.062017
1890.439941	147.672736	48.067021
1886.702469	141.903052	48.072026
1883.529286	138.704431	48.077031
1879.614204	135.650061	48.082036
1876.417799	145.071303	48.087041
1873.316664	132.188261	48.092045
1869.276312	140.041535	48.097050
1866.104201	142.282768	48.102055
1862.162670	138.824883	48.107060
1858.736416	133.145312	48.112065
1854.915942	141.061342	48.117069
1851.678502	144.376435	48.122074
1848.696549	131.278165	48.127079
1844.445319	137.720592	48.132084
1841.075793	130.536041	48.137089
1837.839323	134.223160	48.142093
1834.463732	131.480114	48.147098
1831.135696	132.692946	48.152103
1827.204755	143.689731	48.157108
1823.466851	142.405075	48.162113
1820.327007	130.625670	48.167117
1817.030077	140.982157	48.172122
1813.728898	135.632826	48.177127
1809.637269	136.383544	48.182132
1806.233245	138.097948	48.187137
1802.778848	142.214188	48.192141
1799.106682	137.835681	48.197146
1795.699437	130.989318	48.202151
1792.353301	133.317757	48.207156
1788.755702	132.991708	48.212161
1785.399515	135.230247	48.217165
1781.662121	129.763163	48.222170
1778.241063	126.104328	48.227175
1774.532668	136.458556	48.232180
1771.323511	139.704301	48.237185
1767.594023	134.226252	48.242189
1764.490743	133.872237	48.247194
1761.206791	135.867580	48.252199
1757.143803	143.932675	48.257204
1753.913861	133.311581	48.262209
1750.390276	142.228872	48.267213
1746.843576	139.484557	48.272218
1743.296681	135.122501	48.277223
1739.733328	143.177294	48.282228
1736.232217	136.424629	48.287233
1732.747229	137.530846	48.292237
1729.136049	137.700430	48.297242
1725.844372	137.865779	48.302247
1722.122218	139.884996	48.307252
1718.843942	127.498642	48.312257
1715.108938	135.915899	48.317261
1711.848142	136.596930	48.322266
1708.739351	132.317040	48.327271
1704.882371	131.369866	48.332276
1701.375613	122.595457	48.337281
1697.587820	127.220921	48.342285
1693.625050	136.634883	48.347290
1690.668279	126.968820	48.352295
1687.278140	134.975490	48.357300
1683.933923	128.213527	48.362305
1680.267826	133.586147	48.367309
1676.764004	131.606394	48.372314
1673.324014	126.028896	48.377319
1669.314776	136.131565	48.382324
1666.202991	129.668659	48.387329
1662.871879	134.399854	48.392333
1659.310759	129.276325	48.397338
1655.769506	131.970594	48.402343
1651.916748	134.268575	48.407348
1648.582517	136.623167	48.412353
1645.356658	135.879416	48.417357
1641.680352	132.540116	48.422362
1638.349194	130.039309	48.427367
1634.409768	133.001850	48.432372
1631.236918	135.400437	48.437377
1627.594114	136.471829	48.442381
1623.971932	146.435006	48.447386
1620.830820	127.017625	48.452391
1617.023028	135.100057	48.457396
1613.618458	130.755045	48.462401
1610.198237	134.277704	48.467405
1606.939689	136.979763	48.472410
1603.473197	127.818314	48.477415
1599.784049	144.416201	48.482420
1596.340444	133.709372	48.487425
1592.887604	130.889284	48.492429
1589.013923	134.105628	48.497434
1585.398144	126.020869	48.502439
1582.139540	130.933131	48.507444
1578.606922	125.927900	48.512449
1574.890643	130.399557	48.517453
1571.540853	129.983196	48.522458
1568.483198	132.133088	48.527463
1564.486778	126.840024	48.532468
1560.909652	128.304169	48.537473
1557.774045	121.227618	48.542477
1554.219727	119.802534	48.547482
1550.546216	130.661460	48.552487
1546.955239	133.827176	48.557492
1543.748852	129.928408	48.562497
1540.468943	126.757929	48.567501
1536.910516	126.717068	48.572506
1533.103829	125.962420	48.577511
1529.269547	126.370704	48.582516
1525.949553	126.683744	48.587521
1522.325063	122.630698	48.592525
1519.267676	131.797492	48.597530
1515.959232	117.708544	48.602535
1512.268702	127.331424	48.607540
1508.691617	128.364420	48.612545
1505.322013	123.330929	48.617549
1501.339324	131.574563	48.622554
1498.121149	121.103688	48.627559
1494.433007	127.136625	48.632564
1490.931413	123.639323	48.637569
1487.771062	114.328522	48.642573
1483.757559	121.553867	48.647578
1480.329039	122.799334	48.652583
1477.116140	123.149176	48.657588
1473.470329	119.499895	48.662593
1470.009014	123.289530	48.667597
1466.521097	120.609528	48.672602
1463.274958	122.926206	48.677607
1459.499442	125.943300	48.682612
1456.269991	128.053178	48.687617
1452.648897	115.580444	48.692621
1448.764187	125.156918	48.697626
1445.949778	121.088658	48.702631
1441.812264	128.081350	48.707636
1438.172852	123.509080	48.712641
1435.008414	122.399726	48.717645
1431.571320	121.129811	48.722650
1428.420933	113.239420	48.727655
1424.509101	122.585759	48.732660
1420.856959	118.103425	48.737665
1417.445765	124.221480	48.742669
1413.807380	130.839646	48.747674
1410.415428	120.565102	48.752679
1407.274233	116.943972	48.757684
1403.675737	118.508462	48.762689
1399.934498	129.535171	48.767693
1396.317599	124.905539	48.772698
1393.005854	124.359290	48.777703
1389.652431	125.704894	48.782708
1386.386258	121.670490	48.787713
1382.940312	123.708650	48.792717
1378.967440	126.242391	48.797722
1375.433302	123.571284	48.802727
1371.367933	127.798274	48.807732
1367.944172	130.549704	48.812737
1365.129043	120.555589	48.817741
1361.736563	121.332037	48.822746
1358.159822	115.786870	48.827751
1354.653864	123.845650	48.832756
1350.797355	125.770736	48.837761
1347.185591	126.775447	48.842765
1343.878751	122.664915	48.847770
1340.850075	112.671191	48.852775
1336.940650	120.288133	48.857780
1333.600616	127.644020	48.862785
1330.127069	120.480035	48.867789
1326.231775	130.782972	48.872794
1323.194897	125.218651	48.877799
1319.368737	128.702443	48.882804
1315.938079	124.413877	48.887809
1312.607002	122.894854	48.892813
1309.030897	130.185191	48.897818
1305.122241	126.340322	48.902823
1301.889880	130.866583	48.907828
1298.509085	124.522420	48.912833
1294.861522	122.380833	48.917837
1291.276245	123.906717	48.922842
1287.774500	114.848263	48.927847
1284.173838	134.991661	48.932852
1280.603573	116.028763	48.937857
1277.522495	127.676971	48.942861
1274.034612	128.759338	48.947866
1270.708442	123.721614	48.952871
1266.872180	126.188466	48.957876
1263.642985	133.640534	48.962881
1260.140244	123.774564	48.967885
1256.157244	127.756164	48.972890
1252.699339	121.940427	48.977895
1248.959313	126.158928	48.982900
1245.886211	121.558722	48.987905
1242.517560	119.900723	48.992909
1239.090003	122.964467	48.997914
1235.410553	124.559045	49.002919
1231.624013	137.059575	49.007924
1228.497816	120.692885	49.012929
1224.766292	121.162381	49.017933
1220.674515	135.511508	49.022938
1217.700573	120.155478	49.027943
1214.560859	128.501319	49.032948
1211.262329	127.100326	49.037953
1207.579546	128.502680	49.042957
1203.593925	124.238065	49.047962
1200.728461	122.533616	49.052967
1196.775055	133.466486	49.057972
1193.385988	127.796495	49.062977
1190.106971	123.158342	49.067981
1186.302139	121.643734	49.072986
1182.523357	119.702326	49.077991
1178.765081	124.609840	49.082996
1175.499848	114.855844	49.088001
1172.476516	115.892665	49.093005
1168.839738	125.114987	49.098010
1165.679606	119.786848	49.103015
1161.612220	122.388888	49.108020
1158.324635	127.278196	49.113025
1154.955946	123.200333	49.118029
1151.238840	124.421134	49.123034
1147.841971	110.901253	49.128039
1144.049813	123.872621	49.133044
1140.743587	116.817493	49.138049
1137.625254	124.325900	49.143053
1133.470512	126.560167	49.148058
1130.321492	122.230909	49.153063
1126.708145	122.337779	49.158068
1123.146693	123.275146	49.163073
1119.987835	117.086248	49.168077
1116.370784	117.899216	49.173082
1113.124203	112.412941	49.178087
1109.268963	110.991391	49.183092
1105.864665	121.201071	49.188097
1102.673043	113.356824	49.193101
1098.432894	117.304898	49.198106
1095.520530	115.442512	49.203111
1091.664206	116.003990	49.208116
1088.262876	112.743618	49.213121
1084.483388	119.854812	49.218125
1081.005974	122.936582	49.223130
1077.659798	108.190228	49.228135
1073.889288	116.827719	49.233140
1070.677809	116.074501	49.238145
1067.334354	114.298411	49.243149
1063.423991	116.898647	49.248154
1060.320975	118.283596	49.253159
1056.687147	113.814529	49.258164
1053.051656	120.173963	49.263169
1049.753696	120.764908	49.268173
1046.271989	119.492206	49.273178
1042.831304	112.093728	49.278183
1038.990695	121.838448	49.283188
1035.972551	117.331528	49.288193
1032.206249	122.784538	49.293197
1028.125174	127.460790	49.298202
1025.072600	114.659813	49.303207
1021.554613	119.197177	49.308212
1018.136169	120.528936	49.313217
1015.326560	121.967224	49.318221
1011.253237	129.465891	49.323226
1008.174901	119.988575	49.328231
1004.384994	124.264652	49.333236
1000.328983	124.392134	49.338241
997.088963	119.339790	49.343245
993.340246	119.888294	49.348250
990.173720	128.508660	49.353255
986.519573	126.727173	49.358260
982.988333	115.235775	49.363265
979.674433	121.073214	49.368269
975.833910	123.285064	49.373274
972.531954	117.976776	49.378279
969.167498	123.442119	49.383284
965.833392	127.358294	49.388289
962.217604	125.405906	49.393293
958.615792	123.435424	49.398298
955.255210	121.666591	49.403303
951.446361	123.755808	49.408308
948.169452	122.068457	49.413313
944.472264	116.468177	49.418317
940.945561	119.137284	49.423322
937.664385	118.348722	49.428327
934.230138	125.366628	49.433332
930.181509	120.928179	49.438337
926.707319	122.357237	49.443341
923.549591	128.291040	49.448346
920.429855	118.823009	49.453351
917.079592	121.793887	49.458356
913.548718	118.606384	49.463361
909.848843	118.661039	49.468365
905.980177	121.658262	49.473370
902.224675	113.583207	49.478375
898.812204	117.717418	49.483380
895.158376	113.345926	49.488385
892.257003	105.851083	49.493389
888.764151	112.124096	49.498394
885.247987	113.039162	49.503399
881.552580	120.714206	49.508404
878.000104	119.065774	49.513409
874.259627	112.091170	49.518413
870.476008	118.265274	49.523418
867.610470	117.781775	49.528423
864.460888	117.152658	49.533428
860.573767	121.689426	49.538433
856.983942	112.255391	49.543437
853.160865	116.649357	49.548442
849.916440	104.719335	49.553447
846.461046	120.847043	49.558452
843.260337	110.290549	49.563457
839.459248	112.321150	49.568461
836.096772	104.994968	49.573466
832.554848	97.580861	49.578471
828.890955	110.229104	49.583476
825.443078	110.136772	49.588481
822.058060	109.925905	49.593485
818.556691	115.007091	49.598490
815.201228	109.700875	49.603495
811.418263	107.020077	49.608500
808.116100	116.016215	49.613505
804.414359	114.240782	49.618509
800.725183	116.174760	49.623514
797.685444	110.458960	49.628519
794.166272	103.772642	49.633524
790.632546	103.998828	49.638529
786.843187	110.689384	49.643533
783.293720	109.634710	49.648538
779.999152	113.542499	49.653543
776.030164	112.573209	49.658548
772.684485	108.120661	49.663553
769.605534	111.370198	49.668557
765.896445	104.312558	49.673562
762.618576	111.012062	49.678567
759.248728	126.079997	49.683572
755.375960	113.848462	49.688577
751.717451	107.142604	49.693581
747.995935	110.825432	49.698586
744.928528	107.510690	49.703591
741.375520	114.876737	49.708596
737.942461	113.394162	49.713601
734.533373	119.491025	49.718605
731.118445	115.928303	49.723610
727.506858	110.287616	49.728615
723.793998	106.289137	49.733620
720.547819	110.604551	49.738625
717.206633	108.334425	49.743629
713.142122	111.816498	49.748634
710.101736	104.902259	49.753639
706.286480	112.087935	49.758644
702.824124	106.799297	49.763649
699.273646	106.176826	49.768653
695.635632	113.026925	49.773658
692.228068	106.357949	49.778663
688.944699	112.899164	49.783668
685.276121	107.363453	49.788673
681.847153	101.196893	49.793677
678.189043	112.263829	49.798682
675.012510	102.790405	49.803687
671.091827	114.518247	49.808692
667.942318	113.688175	49.813697
664.504652	110.793500	49.818701
660.531522	122.003543	49.823706
657.321923	113.409397	49.828711
653.654390	126.383980	49.833716
650.382411	113.880883	49.838721
647.033214	109.273123	49.843725
643.188296	125.011532	49.848730
639.835500	104.902117	49.853735
636.230554	110.187250	49.858740
632.835686	106.727656	49.863745
629.722096	112.328541	49.868749
625.896156	110.311157	49.873754
622.302291	106.940340	49.878759
618.638438	118.502992	49.883764
615.572189	110.633460	49.888769
611.594573	109.171029	49.893773
608.266265	112.362078	49.898778
604.805706	112.277541	49.903783
601.166267	106.001815	49.908788
597.783445	102.323978	49.913793
594.406167	107.176410	49.918797
590.635807	110.609135	49.923802
587.302012	116.148999	49.928807
583.993857	110.026860	49.933812
580.302704	111.602196	49.938817
576.759582	110.354436	49.943821
572.953755	118.420945	49.948826
569.498425	104.107721	49.953831
566.356939	113.145904	49.958836
562.696915	110.755591	49.963841
559.273877	108.567804	49.968845
555.303619	108.490682	49.973850
552.540244	100.801381	49.978855
548.941032	111.361380	49.983860
545.235544	113.991898	49.988865
541.717847	104.314354	49.993869
537.945622	112.789533	49.998874
534.641168	106.815220	50.003879
531.089414	110.449018	50.008884
527.764355	109.934625	50.013889
524.595012	112.012116	50.018893
520.934383	112.518026	50.023898
517.274358	112.065580	50.028903
513.717979	111.708863	50.033908
509.997919	106.959525	50.038913
506.511482	98.910776	50.043917
502.728066	111.244740	50.048922
499.692393	113.351437	50.053927
496.092966	110.840450	50.058932
492.736550	111.596584	50.063937
489.136567	107.905830	50.068941
485.857527	106.972412	50.073946
481.875610	104.206430	50.078951
478.682436	111.626788	50.083956
475.047044	112.210848	50.088961
471.773516	105.255057	50.093965
467.984981	107.434263	50.098970
464.882799	111.606046	50.103975
461.105453	114.200375	50.108980
457.642815	110.030681	50.113985
454.308290	103.417311	50.118989
450.720317	114.777688	50.123994
447.231131	105.503007	50.128999
443.469617	105.995682	50.134004
439.661939	108.332000	50.139009
436.405506	103.559484	50.144013
433.326656	108.953466	50.149018
429.911361	106.124153	50.154023
426.323537	107.937472	50.159028
422.650155	107.381349	50.164033
419.108668	102.950246	50.169037
415.647016	113.779435	50.174042
412.312669	101.084218	50.179047
408.624124	103.620283	50.184052
404.842517	101.087429	50.189057
401.582737	100.782951	50.194061
397.885569	105.365627	50.199066
394.454491	99.816529	50.204071
391.304328	101.679397	50.209076
387.598056	99.415293	50.214081
384.024972	95.760833	50.219085
380.406892	110.764690	50.224090
377.413327	99.881668	50.229095
373.551343	103.785380	50.234100
370.125797	105.480719	50.239105
366.887665	108.432058	50.244109
362.883100	105.249023	50.249114
359.853293	103.159710	50.254119
355.745774	103.022806	50.259124
352.145828	107.297768	50.264129
349.092373	100.507925	50.269133
345.478813	111.054065	50.274138
342.223391	98.329670	50.279143
338.239805	102.327934	50.284148
334.733112	96.152238	50.289153
331.515506	99.905920	50.294157
328.271998	100.742554	50.299162
324.768988	106.260486	50.304167
321.333420	98.846793	50.309172
317.221747	100.319479	50.314177
314.014718	97.187812	50.319181
309.990524	101.610973	50.324186
306.800767	97.798214	50.329191
303.595173	97.747691	50.334196
299.870371	97.465797	50.339201
296.434765	99.028670	50.344205
292.792079	99.858587	50.349210
289.515306	100.361737	50.354215
285.807614	107.421606	50.359220
282.532546	105.545416	50.364225
279.208728	109.623967	50.369229
275.577652	107.337844	50.374234
271.827082	103.983009	50.379239
268.609973	103.491797	50.384244
264.829916	103.126529	50.389249
261.308798	101.568734	50.394253
257.802987	109.084598	50.399258
254.580826	108.809525	50.404263
250.712126	103.720159	50.409268
247.515688	107.867039	50.414273
244.173268	105.327343	50.419277
240.118710	105.294854	50.424282
237.010179	100.040597	50.429287
233.463946	106.531506	50.434292
230.257502	98.653131	50.439297
226.565984	103.306445	50.444301
222.759915	99.617283	50.449306
219.077398	99.994067	50.454311
215.610703	106.496293	50.459316
212.405703	103.336741	50.464321
209.222073	94.759598	50.469325
205.385864	118.611051	50.474330
202.066660	98.139738	50.479335
198.787485	107.636459	50.484340
194.546621	107.009701	50.489345
191.426091	102.165157	50.494349
187.589018	103.622305	50.499354
184.068310	102.577378	50.504359
181.098389	105.859778	50.509364
177.571933	97.736056	50.514369
174.079848	106.566123	50.519373
170.495517	102.403996	50.524378
166.851569	91.623889	50.529383
163.240610	97.658277	50.534388
159.579553	101.525357	50.539393
156.529386	95.449867	50.544397
152.887992	97.084613	50.549402
149.308041	90.319739	50.554407
145.934337	93.172320	50.559412
141.914549	107.946645	50.564417
138.926262	103.079853	50.569421
135.446519	103.680461	50.574426
132.118677	98.050562	50.579431
128.326747	102.034253	50.584436
124.905388	99.069642	50.589441
121.169276	97.054620	50.594445
117.444043	104.257633	50.599450
114.334717	91.773688	50.604455
111.215675	98.894890	50.609460
107.330547	109.565297	50.614465
104.244767	96.533409	50.619469
99.887101	105.103687	50.624474
96.632436	94.347599	50.629479
93.296610	94.776019	50.634484
89.490079	101.736769	50.639489
86.395125	89.352690	50.644493
82.910147	98.078042	50.649498
79.374629	95.907104	50.654503
75.803697	98.283076	50.659508
72.082002	100.990671	50.664513
68.603236	95.315170	50.669517
65.419691	96.287114	50.674522
61.221809	100.136007	50.679527
58.087044	100.915767	50.684532
54.871411	88.806060	50.689537
51.199710	96.356644	50.694541
47.709497	101.964624	50.699546
44.338013	95.562163	50.704551
40.765457	96.083892	50.709556
37.254519	98.906789	50.714561
33.765037	95.212942	50.719565
30.323489	98.247935	50.724570
26.536004	96.385558	50.729575
23.123678	94.030878	50.734580
19.360809	106.238663	50.739585
16.303312	98.157612	50.744589
12.920161	92.169342	50.749594
9.262388	89.898336	50.754599
5.704971	100.873503	50.759604
2.085469	91.972466	50.764609