Tue Jun 21 11:24:53 2022

Number of Points = 9931

Depth (nm)	Load (N)	Time (s)
-0.664114	77.428937	0.000000
-0.541390	72.982277	0.005005
-0.859617	83.021250	0.010010
-0.637626	68.732940	0.015014
-0.796640	77.776048	0.020019
-0.839394	66.246292	0.025024
-1.098421	49.201585	0.030029
-1.313529	66.245951	0.035034
-1.796642	50.736303	0.040038
-2.199384	41.239504	0.045043
-2.237887	40.201241	0.050048
-2.911279	28.998927	0.055053
-3.160273	29.661992	0.060058
-3.088276	19.971154	0.065062
-3.606994	26.791451	0.070067
-4.060410	15.493718	0.075072
-4.126773	16.735311	0.080077
-4.632507	32.318765	0.085082
-4.520850	15.245274	0.090086
-4.595337	11.865507	0.095091
-5.421590	19.527831	0.100096
-5.647036	11.032951	0.105101
-5.947555	15.658888	0.110106
-5.583492	15.149119	0.115110
-5.922558	22.594611	0.120115
-6.460667	24.945581	0.125120
-6.678111	8.800776	0.130125
-7.575489	20.102239	0.135130
-7.206929	13.413646	0.140134
-7.506427	26.399005	0.145139
-7.622292	12.241287	0.150144
-7.572037	16.003234	0.155149
-8.555911	18.767431	0.160154
-8.801648	14.829155	0.165158
-8.824240	15.240822	0.170163
-8.943537	22.576316	0.175168
-9.340500	15.211345	0.180173
-9.506680	23.303874	0.185178
-9.547283	11.713420	0.190182
-10.378873	9.608683	0.195187
-10.774122	21.055508	0.200192
-10.524455	7.621068	0.205197
-10.709458	8.138562	0.210202
-10.403473	8.721171	0.215206
-11.315472	12.817297	0.220211
-12.028979	18.046592	0.225216
-11.802802	22.632279	0.230221
-12.366134	20.422340	0.235226
-12.304665	19.011339	0.240230
-12.375156	22.998706	0.245235
-12.871374	18.769995	0.250240
-12.434408	15.431037	0.255245
-13.082163	21.348593	0.260250
-13.615089	21.949551	0.265254
-13.967576	25.476274	0.270259
-14.024078	24.879465	0.275264
-13.780826	21.477864	0.280269
-14.890091	16.231600	0.285274
-15.115913	20.146417	0.290278
-15.473760	27.326254	0.295283
-15.659370	19.188458	0.300288
-15.267759	14.600596	0.305293
-15.559717	23.530119	0.310298
-15.661323	24.832605	0.315302
-16.314304	18.562402	0.320307
-16.527907	17.062963	0.325312
-16.912630	10.983759	0.330317
-17.237289	13.244327	0.335322
-16.538226	3.757301	0.340326
-17.315973	16.914199	0.345331
-17.926838	14.560385	0.350336
-18.165897	13.622428	0.355341
-18.963605	20.298300	0.360346
-18.638042	13.874740	0.365350
-18.712663	15.500130	0.370355
-18.862215	13.105247	0.375360
-19.012932	7.365975	0.380365
-19.727765	15.612698	0.385370
-20.016660	7.135827	0.390374
-20.333879	16.340466	0.395379
-20.217101	14.811182	0.400384
-20.325121	12.100794	0.405389
-20.568570	25.803842	0.410394
-21.098975	14.955165	0.415398
-21.608774	19.204125	0.420403
-21.759800	17.131532	0.425408
-21.634495	15.459348	0.430413
-21.857046	21.458044	0.435418
-21.953814	10.643331	0.440422
-22.629757	12.051580	0.445427
-23.296856	13.798368	0.450432
-23.329895	10.556383	0.455437
-23.498499	13.717978	0.460442
-23.367693	12.333185	0.465446
-23.318842	10.548949	0.470451
-24.268911	20.047827	0.475456
-24.796271	13.226989	0.480461
-25.286394	14.832780	0.485466
-24.699367	13.102488	0.490470
-24.917402	12.903414	0.495475
-24.854140	19.309432	0.500480
-25.038961	18.296585	0.505485
-26.010634	17.741610	0.510490
-26.462086	10.268452	0.515494
-27.115869	15.497921	0.520499
-26.866081	21.329204	0.525504
-26.782071	7.477609	0.530509
-26.616909	9.930763	0.535514
-26.746683	6.009992	0.540518
-27.205055	15.731533	0.545523
-27.775125	16.463160	0.550528
-27.963839	3.148681	0.555533
-28.159160	19.327374	0.560538
-28.231911	12.375608	0.565542
-29.072516	15.446022	0.570547
-29.485310	16.808327	0.575552
-29.450223	17.989312	0.580557
-29.686111	18.019337	0.585562
-29.634898	8.501064	0.590566
-29.909273	7.116277	0.595571
-29.965739	18.610399	0.600576
-30.516409	11.682523	0.605581
-30.716484	13.349999	0.610586
-30.767997	12.229237	0.615590
-31.100657	12.279432	0.620595
-32.075500	16.900217	0.625600
-32.133398	6.928587	0.630605
-32.725997	14.671802	0.635610
-32.608068	12.984264	0.640614
-32.769629	18.902214	0.645619
-32.863210	16.046566	0.650624
-32.784499	6.704497	0.655629
-33.248383	15.860015	0.660634
-33.104280	11.884615	0.665638
-33.489706	8.205880	0.670643
-34.314261	21.493471	0.675648
-34.546162	13.896735	0.680653
-34.618571	15.374352	0.685658
-34.375332	5.559659	0.690662
-35.365607	18.578101	0.695667
-35.543760	7.480280	0.700672
-35.738077	7.458035	0.705677
-36.398881	11.562689	0.710682
-36.436295	11.121573	0.715686
-35.992266	18.069752	0.720691
-36.147454	13.060166	0.725696
-36.465512	18.789136	0.730701
-37.525519	18.027582	0.735706
-37.573065	18.885208	0.740710
-37.675801	18.723873	0.745715
-38.144258	14.068476	0.750720
-37.922726	15.097621	0.755725
-38.186824	21.797017	0.760730
-38.130067	16.650507	0.765734
-38.768537	21.424764	0.770739
-39.273526	19.744280	0.775744
-39.374230	16.506198	0.780749
-39.402963	19.841175	0.785754
-39.635791	13.020306	0.790758
-40.176641	14.257792	0.795763
-40.568460	21.567967	0.800768
-40.441144	13.315605	0.805773
-41.315376	27.823837	0.810778
-40.986549	21.501163	0.815782
-40.905218	12.016972	0.820787
-42.194254	17.527268	0.825792
-41.971397	16.859334	0.830797
-42.496252	23.576653	0.835802
-42.487498	15.784961	0.840806
-42.323491	9.746315	0.845811
-42.544200	15.869417	0.850816
-42.633237	9.330209	0.855821
-43.287416	13.017989	0.860826
-43.737156	9.729572	0.865830
-43.762262	10.764238	0.870835
-44.407010	8.474648	0.875840
-44.277307	-1.164162	0.880845
-44.559020	14.033882	0.885850
-45.169876	6.069328	0.890854
-45.520094	7.854218	0.895859
-45.524001	12.858260	0.900864
-45.205152	11.100942	0.905869
-45.517929	19.714232	0.910874
-45.744886	11.676629	0.915878
-46.346206	18.332807	0.920883
-46.950653	10.567285	0.925888
-47.114104	8.830244	0.930893
-47.316712	14.044988	0.935898
-47.086603	14.516038	0.940902
-46.996277	11.520615	0.945907
-48.003073	15.828595	0.950912
-48.461197	16.319096	0.955917
-48.947917	16.384938	0.960922
-49.008312	11.804639	0.965926
-48.875836	13.289173	0.970931
-48.950477	26.781338	0.975936
-48.900493	21.353172	0.980941
-49.470318	20.546360	0.985946
-50.090166	11.860465	0.990950
-50.038455	20.102794	0.995955
-50.428644	16.994743	1.000960
-50.523698	17.023745	1.005965
-50.790201	15.899120	1.010970
-51.222332	17.578387	1.015974
-51.650867	14.767752	1.020979
-52.167325	17.429688	1.025984
-51.779990	12.806224	1.030989
-52.255015	8.900795	1.035994
-52.182813	11.324153	1.040998
-51.869925	16.344799	1.046003
-53.247559	18.255829	1.051008
-53.325795	11.327667	1.056013
-53.666311	21.751337	1.061018
-53.938838	16.987720	1.066022
-53.802218	14.423892	1.071027
-53.679689	11.491807	1.076032
-53.647630	12.781431	1.081037
-54.748385	19.950897	1.086042
-55.104910	9.605050	1.091046
-55.358368	4.694818	1.096051
-55.461443	20.394305	1.101056
-55.399154	10.050929	1.106061
-56.091093	23.762138	1.111066
-56.059958	11.122237	1.116070
-56.504522	17.927490	1.121075
-56.536886	12.395946	1.126080
-56.467000	12.258909	1.131085
-57.109939	16.563664	1.136090
-57.948784	11.437602	1.141094
-58.315970	9.270768	1.146099
-58.446729	14.225172	1.151104
-57.638593	11.353200	1.156109
-58.176850	18.009789	1.161114
-58.319295	13.843662	1.166118
-58.418600	13.293606	1.171123
-59.388326	19.980012	1.176128
-59.822259	11.966820	1.181133
-60.063353	23.462511	1.186138
-59.903072	19.531789	1.191142
-59.984905	10.394498	1.196147
-60.050128	11.219926	1.201152
-60.055783	4.501943	1.206157
-61.176492	12.906853	1.211162
-61.257928	12.430206	1.216166
-61.567524	10.519246	1.221171
-61.790196	11.352200	1.226176
-61.913430	11.293715	1.231181
-61.714064	13.606227	1.236186
-62.263821	15.671815	1.241190
-62.878893	12.916346	1.246195
-63.258534	15.904902	1.251200
-63.011391	12.888640	1.256205
-63.386411	14.305667	1.261210
-63.510038	13.568622	1.266214
-64.134288	12.588886	1.271219
-64.626951	14.702442	1.276224
-64.741204	3.276736	1.281229
-65.028868	10.936695	1.286234
-65.048574	7.307115	1.291238
-65.135392	13.391072	1.296243
-65.277410	18.166783	1.301248
-64.816608	14.274502	1.306253
-65.936491	15.727664	1.311258
-66.290177	15.487318	1.316262
-66.354848	11.328243	1.321267
-66.716687	12.265544	1.326272
-66.346505	12.825481	1.331277
-67.160306	5.907841	1.336282
-67.635247	15.352901	1.341286
-67.717009	12.500824	1.346291
-67.922753	14.840565	1.351296
-67.761715	11.666094	1.356301
-68.632017	18.518173	1.361306
-69.108692	9.518890	1.366310
-69.343479	11.479432	1.371315
-69.472176	23.859303	1.376320
-69.553865	20.897495	1.381325
-69.742101	17.789943	1.386330
-69.501654	13.087994	1.391334
-69.546143	7.731127	1.396339
-70.445828	22.072681	1.401344
-70.730216	7.220060	1.406349
-71.202906	10.714198	1.411354
-71.248419	12.657208	1.416358
-71.097524	9.838629	1.421363
-71.573649	14.068596	1.426368
-72.170433	19.738351	1.431373
-72.575190	17.385933	1.436378
-72.848765	16.172497	1.441382
-72.735635	21.074476	1.446387
-73.113145	19.272443	1.451392
-72.999249	21.418354	1.456397
-73.253498	14.234197	1.461402
-73.463445	12.095392	1.466406
-74.083783	10.035406	1.471411
-74.520774	9.907721	1.476416
-74.616880	7.080911	1.481421
-74.650621	15.138279	1.486426
-74.914952	15.890319	1.491430
-74.533776	7.108707	1.496435
-75.211922	18.560150	1.501440
-75.855318	15.362218	1.506445
-75.987844	19.819245	1.511450
-76.379052	8.767566	1.516454
-76.170327	12.199966	1.521459
-76.337390	12.467826	1.526464
-77.112989	10.009683	1.531469
-77.997854	18.243329	1.536474
-77.531684	2.014342	1.541478
-77.631106	7.726242	1.546483
-77.761509	9.287856	1.551488
-77.635836	5.400166	1.556493
-78.650633	10.292394	1.561498
-78.735120	6.149824	1.566502
-79.221754	-0.488303	1.571507
-79.431476	4.706896	1.576512
-79.231706	8.291342	1.581517
-79.400558	9.358298	1.586522
-79.801562	9.327463	1.591526
-80.473412	2.330081	1.596531
-81.148047	7.220636	1.601536
-80.558368	-0.737502	1.606541
-80.928995	10.367206	1.611546
-80.850279	0.029209	1.616550
-80.795604	3.446665	1.621555
-81.803904	10.338369	1.626560
-81.756932	11.375700	1.631565
-82.140110	9.889747	1.636570
-82.396457	12.293911	1.641574
-82.660052	15.779865	1.646579
-83.621848	10.661543	1.651584
-83.676650	5.610277	1.656589
-83.911034	9.862763	1.661594
-83.919277	0.683496	1.666598
-83.846687	9.522444	1.671603
-83.778432	8.008891	1.676608
-83.821084	10.091335	1.681613
-84.453686	4.958752	1.686618
-85.042473	10.714599	1.691622
-85.190959	2.644672	1.696627
-85.611219	10.417955	1.701632
-85.271749	8.914541	1.706637
-85.933001	9.520185	1.711642
-86.631859	14.744693	1.716646
-86.709670	10.071575	1.721651
-87.016073	16.165652	1.726656
-86.903580	8.927669	1.731661
-87.357702	14.052643	1.736666
-87.486582	11.721237	1.741670
-87.280150	2.642575	1.746675
-88.320548	13.206814	1.751680
-88.369579	24.636952	1.756685
-88.605103	23.283029	1.761690
-88.950340	19.253693	1.766694
-88.623550	13.003977	1.771699
-88.850717	19.743036	1.776704
-89.509735	15.389551	1.781709
-90.053914	14.570408	1.786714
-90.078268	14.794703	1.791718
-90.422349	9.656764	1.796723
-90.504060	15.365339	1.801728
-90.299024	9.673912	1.806733
-90.602117	20.341797	1.811738
-91.585170	17.485856	1.816742
-91.743365	17.112695	1.821747
-92.168840	24.509747	1.826752
-92.228639	13.623405	1.831757
-92.256599	17.396328	1.836762
-92.106740	17.715697	1.841766
-92.295676	9.640231	1.846771
-92.855244	14.588297	1.851776
-93.466108	4.349111	1.856781
-93.849141	12.263241	1.861786
-94.192813	3.324425	1.866790
-93.604734	22.626191	1.871795
-94.057732	8.514064	1.876800
-94.119536	11.203121	1.881805
-94.675956	16.181648	1.886810
-95.272464	14.531721	1.891814
-95.352472	6.808018	1.896819
-95.409804	17.409546	1.901824
-95.327377	9.102069	1.906829
-96.173198	22.817845	1.911834
-96.489797	11.179971	1.916838
-96.695574	12.984948	1.921843
-97.088602	15.618553	1.926848
-96.955894	14.139909	1.931853
-97.312960	14.969863	1.936858
-96.987077	17.412774	1.941862
-97.474241	10.701326	1.946867
-98.205815	11.291189	1.951872
-98.687764	8.815597	1.956877
-99.087390	16.665385	1.961882
-99.169140	5.198188	1.966886
-98.758420	9.999175	1.971891
-98.925138	17.759478	1.976896
-98.528181	5.421304	1.981901
-99.429113	5.920815	1.986906
-100.053365	6.105739	1.991910
-99.768298	9.721443	1.996915
-100.834677	13.099437	2.006912
-100.516243	17.905585	2.016909
-99.946311	11.210167	2.026906
-98.886364	13.012526	2.036902
-98.709780	12.803953	2.046899
-98.582515	11.554176	2.056896
-97.538266	18.613308	2.066893
-97.630254	14.853370	2.076890
-96.761448	13.128687	2.086886
-95.851917	9.169296	2.096883
-96.006628	12.206583	2.106880
-95.540126	19.023134	2.116877
-94.536574	15.201298	2.126874
-94.340812	19.830178	2.136870
-93.313217	15.716677	2.146867
-93.123047	12.834311	2.156864
-92.961725	14.978536	2.166861
-92.508167	16.804266	2.176858
-91.685809	17.717919	2.186854
-91.420304	17.385751	2.196851
-90.251783	10.778115	2.206848
-90.039216	16.806668	2.216845
-90.241999	13.708020	2.226842
-88.857998	7.684918	2.236838
-88.610696	7.445073	2.246835
-88.393084	12.547895	2.256832
-87.745101	10.741234	2.266829
-87.007935	10.328583	2.276826
-86.999778	14.040323	2.286822
-86.220964	16.389726	2.296819
-85.580263	15.079221	2.306816
-85.508254	10.285232	2.316813
-84.365476	9.814298	2.326810
-83.946110	11.685405	2.336806
-83.657693	11.825029	2.346803
-83.547085	7.057645	2.356800
-82.825560	9.270916	2.366797
-82.582087	10.688058	2.376794
-81.178326	7.114503	2.386790
-80.998526	10.693096	2.396787
-80.824698	12.770839	2.406784
-80.268516	14.858168	2.416781
-79.488197	16.892966	2.426778
-79.643147	12.917813	2.436774
-78.604475	14.216698	2.446771
-77.964453	14.938071	2.456768
-77.930664	14.664037	2.466765
-77.177504	15.020899	2.476762
-76.652156	13.968181	2.486758
-76.511171	13.697931	2.496755
-75.188090	15.741439	2.506752
-75.116787	11.063746	2.516749
-74.884005	15.268999	2.526746
-74.200034	15.286805	2.536742
-73.346166	12.718740	2.546739
-73.268531	8.681162	2.556736
-72.797906	13.183117	2.566733
-71.901912	15.221285	2.576730
-71.588082	15.256329	2.586726
-71.546122	10.278029	2.596723
-70.498363	15.149917	2.606720
-70.188614	11.779473	2.616717
-69.774119	16.289936	2.626714
-68.886926	11.223623	2.636710
-68.593558	11.894920	2.646707
-68.394914	17.638295	2.656704
-67.715787	15.123275	2.666701
-67.270434	13.175904	2.676698
-66.839897	12.896626	2.686694
-65.708472	10.951817	2.696691
-65.654768	8.005906	2.706688
-65.323720	11.067862	2.716685
-64.098567	9.097257	2.726682
-63.980769	5.284993	2.736678
-63.638465	13.040686	2.746675
-63.457186	12.808220	2.756672
-62.643496	21.315116	2.766669
-62.411670	20.600866	2.776666
-61.345534	15.620704	2.786662
-60.702382	15.856095	2.796659
-60.479496	12.383066	2.806656
-60.323687	14.294463	2.816653
-60.059165	18.404364	2.826650
-59.060491	11.100516	2.836646
-58.633973	12.143944	2.846643
-57.790711	14.573373	2.856640
-57.650772	19.748339	2.866637
-57.459755	5.091362	2.876634
-56.691306	14.399446	2.886630
-56.029477	6.827740	2.896627
-55.777843	14.806508	2.906624
-54.931555	15.230147	2.916621
-54.597342	10.330496	2.926618
-54.390431	7.091485	2.936614
-53.127657	0.681446	2.946611
-53.089518	8.213855	2.956608
-53.021418	9.682369	2.966605
-52.006696	4.347764	2.976602
-51.461035	3.973550	2.986598
-51.224737	10.257406	2.996595
-50.597286	8.117664	3.006592
-49.840342	9.003827	3.016589
-49.434119	4.378355	3.026586
-49.544252	5.365035	3.036582
-48.658208	7.636424	3.046579
-48.082245	5.496713	3.056576
-47.682489	3.320782	3.066573
-46.732310	6.926905	3.076570
-46.572647	6.856087	3.086566
-46.368779	2.486212	3.096563
-45.808509	2.390545	3.106560
-44.947960	3.666773	3.116557
-44.646253	9.993936	3.126554
-43.831992	10.418535	3.136550
-43.610028	11.893973	3.146547
-43.341312	14.805618	3.156544
-42.445570	10.107576	3.166541
-41.904220	11.834799	3.176538
-41.893156	10.186572	3.186534
-40.624487	12.256291	3.196531
-40.347282	10.947305	3.206528
-40.136997	8.058251	3.216525
-39.907101	2.319545	3.226522
-39.178846	4.531314	3.236518
-38.411246	4.059493	3.246515
-37.971600	8.317627	3.256512
-37.274549	8.892437	3.266509
-36.901102	8.880070	3.276506
-36.964111	6.573704	3.286502
-36.221709	3.680902	3.296499
-35.466011	6.231134	3.306496
-35.298099	8.708782	3.316493
-34.157821	11.260928	3.326490
-33.751709	13.255552	3.336486
-33.683092	12.993138	3.346483
-33.474418	9.679741	3.356480
-32.974213	4.073307	3.366477
-32.083485	8.973976	3.376474
-31.152431	11.309442	3.386470
-30.684502	9.520948	3.396467
-30.813765	6.853699	3.406464
-30.593352	7.825948	3.416461
-29.746562	15.995823	3.426458
-28.529749	11.379762	3.436454
-28.514577	9.904531	3.446451
-27.962759	8.633254	3.456448
-27.782263	11.563659	3.466445
-27.050654	17.728945	3.476442
-26.275663	13.497640	3.486438
-26.032971	13.026004	3.496435
-25.836486	6.445586	3.506432
-24.438853	13.829929	3.516429
-24.202390	8.406269	3.526426
-24.333292	11.093049	3.536422
-23.847947	11.411878	3.546419
-23.187651	6.035991	3.556416
-22.854366	10.632223	3.566413
-21.357671	11.565222	3.576410
-21.070299	20.486684	3.586406
-21.183149	10.530378	3.596403
-20.882273	13.063857	3.606400
-19.992954	11.880731	3.616397
-19.671237	12.265778	3.626394
-18.984490	9.695562	3.636390
-18.134751	11.566342	3.646387
-18.252829	13.686301	3.656384
-17.816395	10.416791	3.666381
-17.119702	12.299281	3.676378
-16.467516	11.893996	3.686374
-16.084203	12.676461	3.696371
-15.066607	11.318965	3.706368
-14.965792	13.458396	3.716365
-14.976131	14.174852	3.726362
-13.620567	16.669818	3.736358
-13.558274	11.927226	3.746355
-13.267595	6.902996	3.756352
-12.399811	10.902531	3.766349
-11.762601	12.426377	3.776346
-11.592776	9.482377	3.786342
-11.103546	7.488228	3.796339
-9.985475	12.587766	3.806336
-10.175476	12.044929	3.816333
-9.853265	15.226511	3.826330
-8.920113	13.929235	3.836326
-8.365705	10.748664	3.846323
-8.054267	4.030857	3.856320
-7.095506	13.204498	3.866317
-7.114147	10.825779	3.876314
-6.949673	14.398026	3.886310
-5.964642	7.127073	3.896307
-5.528350	7.959449	3.906304
-5.211647	12.783676	3.916301
-4.508513	8.824691	3.926298
-4.202580	10.138235	3.936294
-3.351320	21.012515	3.946291
-2.869955	28.412070	3.956288
-2.921386	33.172390	3.966285
-2.207124	38.915361	3.976282
-1.662058	44.165516	3.986278
-1.213123	62.324042	3.996275
-0.993464	68.655732	4.006272
-0.617040	91.764163	4.016269
-0.013807	113.488125	4.026266
0.000000	121.945847	4.031270
0.299609	135.732722	4.036275
0.714923	143.526559	4.041280
0.547032	159.947725	4.046285
0.898591	170.737601	4.051290
1.410592	170.049410	4.056294
0.971009	185.692709	4.061299
0.888506	177.522361	4.066304
0.989961	184.856701	4.071309
1.172108	175.674211	4.076314
0.974492	187.295238	4.081318
1.150712	183.259814	4.086323
1.116649	184.757342	4.091328
1.166118	199.937633	4.096333
1.521893	203.383028	4.101338
1.673514	213.618183	4.106342
1.343465	211.851870	4.111347
1.313878	193.787467	4.116352
1.440451	206.831875	4.121357
1.479727	209.024312	4.126362
1.504997	219.019318	4.131366
1.557086	204.670809	4.136371
1.647028	205.171394	4.141376
1.338870	191.001741	4.146381
1.434532	195.293161	4.151386
1.467463	198.793199	4.156390
1.367251	204.994498	4.161395
1.400274	207.076673	4.166400
1.710722	215.945429	4.171405
1.597615	217.404939	4.176410
2.165147	219.478132	4.181414
1.391348	195.215735	4.186419
1.687685	187.129073	4.191424
1.366796	194.804886	4.196429
1.459632	204.976163	4.201434
2.177342	214.314426	4.206438
1.753575	211.420669	4.211443
1.979707	203.004629	4.216448
1.511303	199.377866	4.221453
1.738393	199.731814	4.226458
1.874227	199.064471	4.231462
1.213041	201.608514	4.236467
1.705750	189.898237	4.241472
1.734850	200.160775	4.246477
1.638241	197.389264	4.251482
1.661232	193.585227	4.256486
1.658261	212.186523	4.261491
1.853297	215.423710	4.266496
1.972125	228.703063	4.271501
1.640674	219.795628	4.276506
1.763016	207.623730	4.281510
1.688216	227.076597	4.286515
1.943818	224.802453	4.291520
2.103218	231.558106	4.296525
2.236574	221.547560	4.301530
1.651165	205.116368	4.306534
1.654374	213.396042	4.311539
2.110418	220.500790	4.316544
1.750925	232.996802	4.321549
1.942330	229.914742	4.326554
1.798429	226.597729	4.331558
1.830450	240.739416	4.336563
2.081147	225.452626	4.341568
2.040917	228.946237	4.346573
2.083249	219.159150	4.351578
1.986773	225.132114	4.356582
1.667445	230.761323	4.361587
2.079486	221.156724	4.366592
2.049969	228.224268	4.371597
2.038112	228.023214	4.376602
2.315730	229.132876	4.381606
1.515904	236.955309	4.386611
1.845634	229.388598	4.391616
2.200358	231.874139	4.396621
2.115681	220.606758	4.401626
2.030390	229.759107	4.406630
1.725339	227.812236	4.411635
2.072470	229.661839	4.416640
2.311865	236.610463	4.421645
2.397228	220.088507	4.426650
2.108631	235.061174	4.431654
2.179273	231.898667	4.436659
2.188429	229.570216	4.441664
1.951170	235.763239	4.446669
1.720259	224.991899	4.451674
2.186770	239.241606	4.456678
2.032887	250.729540	4.461683
2.557490	256.828777	4.466688
2.394065	263.604748	4.471693
2.340329	247.308855	4.476698
2.312679	238.450164	4.481702
1.993050	236.547935	4.486707
2.243991	254.435311	4.491712
2.561020	254.293460	4.496717
2.536761	262.021618	4.501722
2.578048	263.083589	4.506726
2.306668	250.371824	4.511731
2.364126	240.668652	4.516736
2.064746	257.923926	4.521741
2.504971	267.594505	4.526746
2.413880	259.017249	4.531750
2.144613	269.940782	4.536755
2.393033	262.257278	4.541760
2.423104	262.422441	4.546765
2.591851	265.878101	4.551770
2.606339	261.859768	4.556774
2.416663	268.158195	4.561779
2.511868	268.350856	4.566784
1.754023	269.431294	4.571789
2.027543	261.733965	4.576794
2.543112	258.518891	4.581798
2.657016	265.841736	4.586803
2.577792	261.008929	4.591808
2.431429	274.518914	4.596813
2.473296	264.798181	4.601818
2.668412	267.277399	4.606822
2.386503	278.504560	4.611827
2.894962	281.272496	4.616832
2.902284	281.403933	4.621837
2.550358	275.082585	4.626842
2.572733	271.574437	4.631846
2.497718	280.489891	4.636851
2.505176	288.400673	4.641856
2.886266	299.819395	4.646861
2.558788	292.236765	4.651866
2.543984	298.096775	4.656870
2.505099	301.150120	4.661875
2.731427	292.117522	4.666880
2.824923	291.066658	4.671885
2.543854	299.744118	4.676890
3.114471	294.271477	4.681894
2.939270	299.722331	4.686899
3.000871	288.533293	4.691904
2.783723	296.201647	4.696909
2.876404	295.746873	4.701914
3.007764	302.179622	4.706918
2.762449	301.089549	4.711923
3.042639	300.539985	4.716928
2.789722	298.508892	4.721933
3.074663	302.581925	4.726938
3.189366	297.513145	4.731942
2.787685	300.766476	4.736947
3.162226	301.980272	4.741952
2.828149	302.479638	4.746957
2.720218	304.402828	4.751962
3.067525	298.959073	4.756966
2.726012	301.779156	4.761971
2.639191	295.038765	4.766976
2.735725	312.705896	4.771981
2.814712	304.567547	4.776986
3.229059	308.405437	4.781990
2.947404	309.982654	4.786995
3.021955	311.121213	4.792000
2.994476	302.002566	4.797005
2.782329	315.511245	4.802010
3.401755	320.747445	4.807014
3.200243	330.919594	4.812019
3.564337	317.933624	4.817024
2.899497	314.504137	4.822029
2.759207	324.883806	4.827034
3.411832	328.057873	4.832038
3.266122	337.064395	4.837043
3.473494	330.238569	4.842048
3.042064	331.922287	4.847053
3.006393	333.619011	4.852058
3.447224	333.111913	4.857062
3.510568	347.716987	4.862067
3.208379	332.165650	4.867072
3.012794	328.565905	4.872077
3.123328	336.522791	4.877082
3.650617	344.308845	4.882086
3.184064	351.607473	4.887091
3.562627	332.992439	4.892096
3.583964	345.112504	4.897101
3.528647	334.085665	4.902106
3.208663	320.258652	4.907110
2.891389	331.078288	4.912115
3.052004	324.812157	4.917120
3.260961	334.753930	4.922125
3.134487	333.143533	4.927130
3.081039	337.815481	4.932134
2.984710	339.091662	4.937139
3.471168	338.777700	4.942144
3.388552	341.318708	4.947149
3.174080	337.264070	4.952154
3.746340	346.877117	4.957158
3.592184	348.553206	4.962163
3.439649	335.313155	4.967168
3.302337	351.722751	4.972173
3.469865	361.498337	4.977178
3.796181	359.430522	4.982182
3.598432	370.609477	4.987187
4.169945	360.909908	4.992192
3.578350	363.744576	4.997197
3.292566	343.464101	5.002202
3.261976	341.295150	5.007206
3.209610	361.898101	5.012211
3.405536	367.303902	5.017216
3.373913	365.422836	5.022221
3.299167	370.736902	5.027226
3.676568	366.980106	5.032230
3.621287	380.178899	5.037235
3.918312	364.986521	5.042240
3.653954	372.940778	5.047245
3.470340	378.357137	5.052250
4.001689	378.076392	5.057254
3.786125	370.883679	5.062259
3.611926	370.659973	5.067264
3.929639	370.764088	5.072269
3.444424	370.876838	5.077274
3.627536	368.223950	5.082278
3.776932	377.359231	5.087283
3.825889	388.844068	5.092288
3.853665	399.835131	5.097293
4.035430	403.056795	5.102298
3.632894	390.670926	5.107302
3.852965	408.052685	5.112307
4.108268	397.612160	5.117312
3.986697	406.144075	5.122317
4.114309	407.393638	5.127322
3.998126	382.203497	5.132326
3.395510	382.889415	5.137331
3.714562	399.813924	5.142336
3.942600	404.166955	5.147341
3.988265	410.095535	5.152346
4.180578	405.003607	5.157350
4.201075	410.730335	5.162355
4.254762	404.504769	5.167360
4.324777	414.113605	5.172365
3.873074	396.993659	5.177370
4.172534	404.946923	5.182374
3.875272	412.918094	5.187379
3.983312	410.916411	5.192384
3.888271	416.630305	5.197389
3.629100	411.613136	5.202394
4.174282	410.821167	5.207398
3.994175	415.715396	5.212403
4.063634	409.874195	5.217408
3.851291	419.204972	5.222413
4.275285	409.707208	5.227418
4.293442	410.992854	5.232422
3.788068	415.770050	5.237427
3.779177	396.697930	5.242432
4.100092	412.077389	5.247437
4.140626	417.155903	5.252442
4.160175	416.012490	5.257446
4.107949	430.653356	5.262451
4.232514	434.921901	5.267456
4.354838	437.476152	5.272461
4.540129	430.245055	5.277466
4.420017	435.287028	5.282470
4.174811	436.904991	5.287475
4.747822	429.091089	5.292480
4.228354	432.219698	5.297485
4.354817	435.530249	5.302490
4.601317	430.761657	5.307494
4.013485	438.435024	5.312499
4.384210	432.975899	5.317504
4.339680	440.427678	5.322509
3.967445	438.356728	5.327514
4.260524	431.060223	5.332518
4.292199	434.865804	5.337523
4.333389	426.810018	5.342528
4.296871	437.137847	5.347533
4.411730	433.431614	5.352538
4.205982	434.685861	5.357542
4.293106	431.790740	5.362547
4.508217	428.575657	5.367552
4.412001	435.749457	5.372557
4.654485	439.619984	5.377562
4.659643	430.889151	5.382566
4.293209	436.641479	5.387571
4.463884	449.957628	5.392576
4.427903	469.374968	5.397581
4.409703	463.769675	5.402586
4.897300	463.651874	5.407590
4.867378	472.292183	5.412595
5.019357	458.347821	5.417600
4.655351	454.031182	5.422605
4.626164	465.390682	5.427610
4.903276	457.688714	5.432614
4.506408	458.754382	5.437619
5.145094	442.805593	5.442624
4.916588	442.440112	5.447629
4.735453	444.099761	5.452634
4.561756	434.808502	5.457638
4.231663	443.641571	5.462643
4.857473	453.590567	5.467648
4.596730	470.759757	5.472653
4.806696	463.202109	5.477658
5.129890	464.908491	5.482662
5.041119	470.066056	5.487667
5.123899	460.654955	5.492672
4.674620	440.496346	5.497677
4.649997	444.301976	5.502682
4.918800	454.301604	5.507686
4.779267	464.808128	5.512691
4.772077	456.258311	5.517696
4.910261	465.132252	5.522701
4.806367	468.603701	5.527706
5.119318	463.466518	5.532710
4.996714	478.674392	5.537715
5.243228	465.579105	5.542720
4.936729	464.220905	5.547725
5.022860	470.177539	5.552730
5.095457	462.456942	5.557734
4.918880	463.279323	5.562739
5.041405	470.321801	5.567744
4.800000	466.179433	5.572749
4.929095	479.239637	5.577754
4.971181	460.881452	5.582758
5.015032	472.435081	5.587763
5.017598	463.160006	5.592768
5.116922	474.365621	5.597773
4.963798	474.477450	5.602778
5.106888	465.695143	5.607782
4.777784	478.140932	5.612787
4.702105	470.169993	5.617792
4.694794	472.984495	5.622797
5.131382	482.106816	5.627802
5.234758	489.730675	5.632806
5.079264	499.181936	5.637811
5.481131	500.533109	5.642816
5.253833	499.613893	5.647821
5.302798	492.877572	5.652826
5.223088	484.306201	5.657830
4.985060	493.255479	5.662835
5.268045	498.061210	5.667840
5.368859	497.744602	5.672845
5.366258	502.049023	5.677850
5.661141	497.453951	5.682854
4.988725	496.223434	5.687859
5.287957	490.150368	5.692864
5.056231	502.329827	5.697869
5.380659	501.210517	5.702874
5.388007	509.287983	5.707878
5.169708	505.277744	5.712883
5.527714	497.688263	5.717888
5.289683	503.767657	5.722893
5.275651	492.484038	5.727898
5.137346	504.644279	5.732902
4.691114	503.510697	5.737907
5.197147	498.784752	5.742912
5.154208	512.770178	5.747917
5.392220	522.460786	5.752922
5.636185	521.215477	5.757926
5.533931	536.258023	5.762931
5.452794	530.168794	5.767936
5.358309	525.453874	5.772941
5.230354	535.988722	5.777946
5.638676	531.713291	5.782950
5.571531	537.009579	5.787955
5.854947	539.885672	5.792960
5.696366	538.359308	5.797965
5.445707	538.012886	5.802970
5.669519	529.285456	5.807974
5.705766	538.942191	5.812979
6.089743	533.536881	5.817984
5.763405	527.413070	5.822989
5.479295	534.620397	5.827994
5.658397	523.987765	5.832998
5.537816	536.448800	5.838003
5.618297	528.285221	5.843008
5.564397	533.320998	5.848013
5.714525	531.127819	5.853018
5.667328	531.438392	5.858022
5.439430	535.899914	5.863027
5.765906	527.205609	5.868032
5.385421	531.559391	5.873037
5.680784	528.154183	5.878042
6.181384	526.232920	5.883046
5.983103	528.629912	5.888051
5.824946	533.809447	5.893056
5.485941	541.765889	5.898061
5.607531	536.806795	5.903066
5.873335	544.963438	5.908070
5.779859	550.539181	5.913075
6.079970	559.749468	5.918080
6.092473	546.278450	5.923085
5.746153	548.066303	5.928090
5.593785	542.239090	5.933094
5.922737	561.101387	5.938099
6.103302	558.797193	5.943104
5.966886	566.177023	5.948109
5.826279	563.615201	5.953114
5.992929	564.501918	5.958118
5.862630	567.725955	5.963123
6.071848	555.872705	5.968128
6.347469	560.656389	5.973133
6.237681	563.472878	5.978138
6.255162	563.866280	5.983142
5.945600	565.228900	5.988147
5.841011	552.820402	5.993152
6.226028	558.938138	5.998157
6.061776	550.988533	6.003162
6.037116	549.419469	6.008166
5.950105	555.422961	6.013171
5.875704	561.489885	6.018176
6.176987	558.699782	6.023181
6.132594	566.263292	6.028186
6.387965	561.156333	6.033190
6.027546	568.649628	6.038195
6.083313	562.149549	6.043200
6.364214	570.115049	6.048205
6.189148	566.410419	6.053210
6.499224	554.772144	6.058214
6.244992	561.115321	6.063219
6.120254	564.538145	6.068224
5.925931	556.465641	6.073229
6.524588	561.240827	6.078234
6.528040	557.970779	6.083238
5.944599	565.370166	6.088243
6.401222	556.601012	6.093248
6.123508	558.589645	6.098253
6.118218	559.619290	6.103258
6.578626	561.729609	6.108262
5.950839	561.881952	6.113267
6.203318	556.682132	6.118272
6.206410	562.583680	6.123277
6.188077	566.761665	6.128282
6.170410	557.153617	6.133286
5.948984	559.476497	6.138291
6.194706	564.514965	6.143296
6.238449	570.163900	6.148301
6.053223	564.280747	6.153306
6.224280	557.214556	6.158310
6.086253	565.438080	6.163315
6.027855	564.189752	6.168320
5.797894	562.832090	6.173325
5.842199	565.711275	6.178330
6.135530	560.912786	6.183334
5.933249	569.051242	6.188339
6.306831	564.382732	6.193344
6.020698	569.861720	6.198349
6.063477	577.927829	6.203354
6.320440	579.353919	6.208358
6.417259	572.632925	6.213363
6.333019	565.492772	6.218368
6.243136	565.304830	6.223373
6.366255	558.350377	6.228378
6.270342	555.158748	6.233382
6.214495	562.505698	6.238387
6.414311	553.715329	6.243392
6.366361	561.556096	6.248397
6.373564	558.353311	6.253402
6.643473	554.541057	6.258406
6.178201	560.844192	6.263411
6.487086	562.191627	6.268416
6.372021	568.530905	6.273421
6.354493	570.531513	6.278426
6.295877	552.682651	6.283430
6.260421	559.482949	6.288435
6.156922	563.312721	6.293440
6.244159	563.442372	6.298445
5.944348	555.782213	6.303450
6.213416	563.146205	6.308454
5.971176	566.015216	6.313459
6.168652	559.174549	6.318464
6.104430	572.181396	6.323469
6.213258	561.321594	6.328474
6.046283	557.177533	6.333478
5.847641	571.623138	6.338483
6.243444	558.523970	6.343488
5.852183	562.272727	6.348493
5.832675	566.953727	6.353498
6.144666	555.607394	6.358502
6.131872	559.061211	6.363507
6.104092	555.829094	6.368512
6.335301	559.855245	6.373517
5.782337	561.972340	6.378522
6.380923	553.434247	6.383526
6.162984	567.086781	6.388531
6.155449	564.169815	6.393536
5.835641	563.166652	6.398541
5.896223	587.708444	6.403546
6.487480	588.678184	6.408550
6.402777	599.810957	6.413555
6.336010	579.295776	6.418560
6.063152	574.564990	6.423565
6.388306	561.486004	6.428570
6.244320	559.888152	6.433574
5.879139	568.209086	6.438579
6.319911	570.358771	6.443584
6.315539	561.690420	6.448589
5.963688	567.705408	6.453594
6.311076	580.678835	6.458598
6.152649	580.516058	6.463603
6.256902	576.269258	6.468608
6.387762	571.961614	6.473613
6.182583	569.155916	6.478618
6.368265	556.542464	6.483622
6.184509	561.850966	6.488627
6.342988	561.063429	6.493632
6.289141	563.142868	6.498637
5.928647	568.834270	6.503642
6.474432	564.583626	6.508646
6.402673	565.368921	6.513651
6.523634	568.711592	6.518656
6.576151	559.149940	6.523661
6.269288	560.575458	6.528666
6.160623	563.606664	6.533670
6.040712	568.982742	6.538675
6.155653	558.124496	6.543680
6.368119	560.198909	6.548685
6.418844	566.131447	6.553690
6.474785	563.200419	6.558694
6.061705	566.462796	6.563699
6.396084	558.253803	6.568704
6.382968	559.320857	6.573709
5.868624	567.456324	6.578714
6.716708	560.432539	6.583718
6.143643	566.485736	6.588723
6.180474	569.189343	6.593728
6.334979	565.476119	6.598733
6.215261	564.168679	6.603738
6.306178	567.348389	6.608742
6.430728	575.157638	6.613747
6.543147	546.716887	6.618752
5.988694	548.213989	6.623757
5.832000	543.509562	6.628762
6.390757	544.522768	6.633766
6.047193	555.551751	6.638771
5.997520	558.015112	6.643776
6.296883	568.998028	6.648781
6.088791	567.730284	6.653786
6.159077	570.220158	6.658790
6.161850	575.007191	6.663795
6.369478	564.604642	6.668800
6.337278	568.709342	6.673805
6.085555	570.931467	6.678810
6.526544	564.126845	6.683814
6.309546	557.823492	6.688819
6.145488	548.940837	6.693824
5.752656	548.040148	6.698829
5.895484	556.908440	6.703834
6.246784	562.038553	6.708838
5.988797	569.918050	6.713843
6.118338	569.207135	6.718848
5.925411	565.728061	6.723853
6.034832	573.458115	6.728858
6.187193	569.798527	6.733862
6.186065	576.023626	6.738867
6.322417	574.256607	6.743872
6.458126	569.631826	6.748877
6.192039	584.671947	6.753882
6.354949	574.615035	6.758886
6.272876	581.122909	6.763891
6.311345	576.232427	6.768896
6.283586	573.608503	6.773901
6.111564	587.015853	6.778906
6.181505	578.846691	6.783910
5.888774	580.586798	6.788915
6.247574	578.505089	6.793920
5.896541	578.807563	6.798925
5.829314	581.672263	6.803930
6.414463	576.881492	6.808934
6.081408	580.613905	6.813939
6.290845	575.457517	6.818944
6.456126	578.100584	6.823949
6.366998	576.129753	6.828954
6.381632	569.655428	6.833958
6.164050	576.696255	6.838963
6.349509	577.518288	6.843968
6.011428	575.129078	6.848973
6.220029	576.350641	6.853978
6.227920	581.050591	6.858982
5.933666	579.985375	6.863987
6.095158	577.825434	6.868992
6.080297	572.590349	6.873997
5.799911	582.142264	6.879002
5.966985	576.636692	6.884006
6.041628	584.027166	6.889011
5.812880	575.081206	6.894016
5.733932	581.007989	6.899021
6.286038	590.500992	6.904026
6.530428	590.211323	6.909030
6.192859	596.948194	6.914035
6.538196	572.138359	6.919040
6.441390	573.175068	6.924045
5.798816	574.966395	6.929050
6.140952	572.895143	6.934054
6.290411	579.703705	6.939059
6.248262	564.378245	6.944064
6.093231	571.530668	6.949069
5.703538	576.097732	6.954074
6.096408	588.847549	6.959078
6.494749	599.377186	6.964083
6.438373	600.816485	6.969088
6.456050	577.910366	6.974093
6.091242	581.191789	6.979098
6.566409	578.191930	6.984102
6.384463	575.645634	6.989107
6.271307	578.134114	6.994112
6.503237	578.831627	6.999117
6.287812	584.841397	7.004122
6.365266	571.040505	7.009126
5.780336	578.140978	7.014131
5.943354	579.100326	7.019136
5.992416	571.259052	7.024141
6.196254	575.223434	7.029146
6.189594	572.898339	7.034150
6.033168	572.578938	7.039155
6.152968	566.819328	7.044160
6.089847	564.420702	7.049165
6.286105	579.551799	7.054170
6.425457	571.961982	7.059174
6.266770	578.263296	7.064179
6.225446	574.786151	7.069184
6.109841	578.429867	7.074189
5.882099	569.555969	7.079194
6.149485	572.440840	7.084198
6.080031	576.763063	7.089203
6.167117	573.926334	7.094208
6.485414	576.666019	7.099213
5.984861	578.282667	7.104218
6.265629	575.268032	7.109222
6.428237	574.932704	7.114227
6.443394	568.942760	7.119232
6.574368	575.006466	7.124237
6.114809	582.237934	7.129242
6.230730	574.689095	7.134246
5.786710	576.907937	7.139251
6.273043	577.434066	7.144256
6.368041	570.916831	7.149261
6.310170	581.328609	7.154266
6.555779	581.747384	7.159270
6.421443	584.698187	7.164275
6.360560	577.950615	7.169280
6.516579	582.167618	7.174285
6.243009	576.279158	7.179290
6.384002	570.676080	7.184294
6.039129	584.646446	7.189299
6.342838	575.626327	7.194304
6.557115	571.442416	7.199309
6.123635	578.137537	7.204314
6.245201	565.228622	7.209318
6.133721	579.873915	7.214323
6.322746	585.518138	7.219328
6.526011	572.780200	7.224333
6.203739	568.161596	7.229338
6.269107	543.600439	7.234342
6.004167	556.264579	7.239347
6.075532	549.452298	7.244352
6.251199	552.013522	7.249357
6.230021	560.183160	7.254362
5.965338	554.886635	7.259366
6.351771	567.485351	7.264371
6.059449	569.243347	7.269376
6.360241	569.754812	7.274381
5.966380	571.371355	7.279386
6.050787	566.204099	7.284390
5.837670	579.258893	7.289395
6.745885	581.123377	7.294400
6.148152	579.825824	7.299405
6.263638	585.076297	7.304410
6.334238	572.714551	7.309414
6.182312	584.106105	7.314419
6.283874	564.767433	7.319424
6.117397	546.452169	7.324429
5.838178	561.582258	7.329434
6.181787	553.445741	7.334438
6.388967	561.612298	7.339443
6.607821	559.120409	7.344448
6.279595	548.187944	7.349453
6.083240	542.555092	7.354458
6.077304	543.285479	7.359462
6.151332	556.079777	7.364467
6.305800	560.091008	7.369472
6.160999	557.813064	7.374477
5.975193	553.128255	7.379482
5.925808	558.352343	7.384486
5.930149	565.555138	7.389491
5.994629	571.091906	7.394496
6.317853	575.313188	7.399501
6.210969	569.895806	7.404506
6.634516	566.516725	7.409510
6.680548	572.849655	7.414515
6.042061	564.294593	7.419520
6.347688	561.313142	7.424525
6.179241	551.092858	7.429530
6.213039	544.974329	7.434534
5.909400	549.182187	7.439539
6.171148	562.526766	7.444544
6.166181	557.316690	7.449549
6.167532	568.091425	7.454554
6.491760	567.916610	7.459558
6.540140	566.858398	7.464563
5.805854	554.896948	7.469568
6.143546	551.892231	7.474573
6.296861	560.205449	7.479578
6.264347	556.799273	7.484582
6.187563	551.141882	7.489587
6.101472	556.071698	7.494592
6.230486	549.768478	7.499597
6.081284	567.256952	7.504602
6.233344	566.289912	7.509606
6.226054	564.919651	7.514611
6.232121	562.478191	7.519616
5.909208	563.943664	7.524621
6.149312	578.452196	7.529626
6.252320	565.547932	7.534630
6.274111	569.953515	7.539635
6.140391	569.416043	7.544640
6.607764	570.876753	7.549645
6.109378	569.208329	7.554650
6.242023	557.405054	7.559654
6.451631	559.975261	7.564659
5.991625	548.398203	7.569664
6.069689	544.854921	7.574669
6.168718	565.773088	7.579674
6.591752	557.101061	7.584678
5.995366	546.736147	7.589683
6.054050	559.137521	7.594688
6.209679	549.888159	7.599693
6.137507	570.469012	7.604698
6.329828	567.283723	7.609702
6.116687	562.485034	7.614707
6.128857	565.173779	7.619712
6.227380	567.372441	7.624717
6.033849	571.197783	7.629722
6.348406	564.590124	7.634726
6.373601	570.546822	7.639731
5.846199	567.478147	7.644736
6.073673	569.495019	7.649741
6.064738	574.131250	7.654746
6.115015	559.015852	7.659750
6.244121	561.200766	7.664755
6.088814	564.616811	7.669760
6.192487	569.234788	7.674765
6.225760	577.328718	7.679770
6.419793	566.119129	7.684774
5.921733	572.264696	7.689779
6.117538	570.190639	7.694784
6.567765	560.252320	7.699789
5.954218	567.901394	7.704794
6.275888	563.614057	7.709798
6.199318	561.145827	7.714803
6.177917	569.654733	7.719808
6.124582	560.095807	7.724813
6.036939	566.098816	7.729818
6.402963	563.616104	7.734822
6.458521	563.502749	7.739827
6.581271	568.609731	7.744832
6.482154	561.966773	7.749837
5.816116	569.279393	7.754842
6.418575	567.652857	7.759846
6.152750	566.960642	7.764851
6.178106	553.505250	7.769856
6.325530	569.786229	7.774861
6.283361	572.382343	7.779866
6.035457	549.650488	7.784870
5.876001	560.630636	7.789875
6.257859	574.091697	7.794880
6.273920	559.064256	7.799885
6.468987	572.485600	7.804890
6.527595	556.890080	7.809894
6.180513	556.316502	7.814899
5.909672	551.725105	7.819904
6.163989	544.698019	7.824909
6.057673	550.241946	7.829914
6.140685	556.133415	7.834918
6.180867	567.496698	7.839923
6.123944	569.444430	7.844928
6.299063	562.292313	7.849933
6.338558	568.307423	7.854938
6.335695	557.352846	7.859942
6.196857	550.192732	7.864947
6.012753	542.292202	7.869952
6.480980	553.320358	7.874957
6.373266	555.869108	7.879962
6.106671	541.009458	7.884966
6.117018	539.433612	7.889971
5.900150	534.850253	7.894976
6.503651	556.244722	7.899981
5.969752	564.936765	7.904986
6.348245	553.784654	7.909990
6.214218	550.835552	7.914995
6.410802	557.486521	7.920000
6.060515	548.671014	7.925005
5.803623	542.112997	7.930010
6.433589	560.148130	7.935014
6.272440	571.777812	7.940019
6.282349	556.168452	7.945024
6.397814	551.865336	7.950029
6.138029	550.648581	7.955034
6.263705	542.055205	7.960038
6.080853	538.645905	7.965043
6.052544	539.730471	7.970048
6.234488	539.809709	7.975053
5.653725	550.821527	7.980058
6.226336	563.428681	7.985062
6.538843	572.067401	7.990067
6.195047	572.265664	7.995072
6.262295	555.718328	8.000077
6.237971	564.502017	8.005082
6.212452	546.023893	8.010086
6.057386	558.019805	8.015091
6.127467	571.364556	8.020096
6.325190	566.384755	8.025101
6.295018	570.611076	8.030106
6.204433	559.660436	8.035123
6.143988	558.876449	8.040141
6.172898	553.039656	8.045158
6.370885	562.524707	8.050176
6.005110	564.214132	8.055194
6.177246	561.562830	8.060211
6.144262	567.608043	8.065229
6.337017	568.449919	8.070246
6.294407	573.465504	8.075264
5.995406	582.009908	8.080282
6.408403	573.867149	8.085299
6.276932	574.902664	8.090317
6.314780	574.005557	8.095334
6.710381	561.950225	8.100352
6.483346	556.732541	8.105370
6.204742	549.029293	8.110387
6.206312	546.376516	8.115405
6.126074	552.320107	8.120422
6.212562	545.920280	8.125440
6.192327	553.361302	8.130458
6.276212	562.376308	8.135475
6.409267	563.172561	8.140493
6.041972	573.539749	8.145510
6.132009	565.265645	8.150528
6.475561	572.799575	8.155546
6.474740	571.858088	8.160563
6.382449	580.768429	8.165581
6.401379	576.667995	8.170598
6.617051	563.181933	8.175616
6.064149	562.875723	8.180634
5.865669	565.062800	8.185651
6.335347	570.781489	8.190669
6.145232	574.313934	8.195686
6.427174	576.412209	8.200704
6.292245	579.500312	8.205722
6.455754	568.568958	8.210739
6.223091	572.199386	8.215757
6.164989	573.919551	8.220774
6.544819	577.792627	8.225792
6.144241	579.316373	8.230810
6.269385	575.847517	8.235827
6.525031	572.218085	8.240845
6.548553	580.599837	8.245862
6.568453	575.667414	8.250880
6.216795	582.097267	8.255898
6.219324	572.574749	8.260915
6.342085	574.309254	8.265933
5.871148	578.873759	8.270950
6.208279	573.510487	8.275968
6.092982	587.004818	8.280986
6.436726	595.203443	8.286003
6.843017	598.498562	8.291021
6.478371	596.246945	8.296038
6.309132	582.488210	8.301056
6.455819	594.178073	8.306074
6.601798	592.601296	8.311091
6.706756	582.434494	8.316109
6.095144	578.988628	8.321126
6.443328	597.986916	8.326144
6.478434	600.288261	8.331162
6.563110	593.446423	8.336179
6.792617	600.424884	8.341197
6.637349	592.584271	8.346214
6.657037	576.501116	8.351232
6.559952	576.423144	8.356250
6.516420	575.506444	8.361267
6.359058	575.937236	8.366285
6.490869	586.267451	8.371302
6.694417	581.272335	8.376320
6.516674	576.575774	8.381338
6.434896	588.994949	8.386355
6.532159	586.343050	8.391373
6.224412	607.501589	8.396390
6.912839	597.259616	8.401408
6.295636	600.691737	8.406426
6.855974	602.887213	8.411443
6.623625	602.534417	8.416461
6.663971	598.488695	8.421478
6.678137	591.410914	8.426496
6.501546	589.110639	8.431514
6.653339	594.337920	8.436531
6.988919	605.349905	8.441549
6.406480	596.258860	8.446566
6.680009	582.106358	8.451584
6.696670	586.861955	8.456602
6.405958	580.614528	8.461619
6.600954	591.126396	8.466637
6.399093	599.709640	8.471654
6.587463	602.734962	8.476672
6.734217	609.861766	8.481690
6.619789	610.885801	8.486707
6.670097	610.548006	8.491725
6.731936	601.024310	8.496742
6.785115	605.258351	8.501760
6.509059	608.352508	8.506778
6.599171	606.340131	8.511795
6.877261	606.627562	8.516813
6.367104	602.738347	8.521830
6.359287	599.331263	8.526848
6.717118	604.987783	8.531866
6.716740	609.748570	8.536883
6.956172	608.381891	8.541901
6.681225	608.838454	8.546918
6.637911	605.361268	8.551936
6.733183	609.233051	8.556954
6.774031	600.921800	8.561971
6.585268	606.229295	8.566989
6.605031	606.284523	8.572007
6.708451	604.821477	8.577024
6.612614	606.993532	8.582042
6.673114	613.202010	8.587059
6.857068	612.720243	8.592077
6.470427	607.465589	8.597095
6.957652	609.225370	8.602112
6.932664	606.341958	8.607130
6.641172	607.969090	8.612147
6.645982	599.450634	8.617165
6.975015	604.766278	8.622183
6.848115	603.655325	8.627200
6.767299	606.650228	8.632218
6.646318	596.890685	8.637235
6.822924	598.300747	8.642253
6.616076	608.384715	8.647271
6.914960	620.505268	8.652288
7.149069	631.027024	8.657306
6.969729	622.694353	8.662323
7.085016	610.260430	8.667341
6.999876	605.148752	8.672359
6.890208	601.828804	8.677376
6.799241	596.303162	8.682394
6.749512	604.456916	8.687411
6.831977	602.559577	8.692429
6.842512	614.047606	8.697447
7.034652	606.262246	8.702464
6.860598	604.579222	8.707482
6.658664	608.173273	8.712499
7.054406	609.925172	8.717517
6.711155	628.154000	8.722535
6.966193	626.403266	8.727552
7.133203	635.662799	8.732570
6.765911	635.824439	8.737587
6.732472	627.581771	8.742605
7.016430	632.999173	8.747623
7.048893	636.437693	8.752640
6.884667	639.938702	8.757658
6.958651	638.144134	8.762675
7.275296	633.870379	8.767693
6.860594	637.988809	8.772711
7.089045	636.690477	8.777728
7.330577	635.647047	8.782746
6.764671	626.997900	8.787763
6.804859	631.160089	8.792781
6.569648	635.461773	8.797799
7.010744	635.416526	8.802816
6.997722	633.839894	8.807834
6.794302	636.499814	8.812851
6.912428	634.423546	8.817869
6.878081	631.698557	8.822887
6.996875	638.489871	8.827904
6.967096	632.030723	8.832922
6.937774	644.637109	8.837939
7.077527	630.505928	8.842957
6.989804	631.219068	8.847975
7.137274	636.624822	8.852992
6.969548	638.100174	8.858010
6.975143	635.403411	8.863027
7.215651	632.087868	8.868045
7.007795	640.830778	8.873063
7.063877	635.567564	8.878080
6.895054	630.419344	8.883098
6.767574	640.384882	8.888115
7.192194	650.325339	8.893133
7.418560	667.482791	8.898151
7.503387	649.577872	8.903168
7.206236	641.293832	8.908186
7.289430	640.203792	8.913203
7.289546	636.247786	8.918221
6.784939	635.420620	8.923239
6.733201	636.101622	8.928256
7.454700	639.805743	8.933274
7.173594	650.867912	8.938291
7.288667	645.770111	8.943309
7.304634	637.875335	8.948327
7.298508	634.455366	8.953344
7.110690	628.770172	8.958362
7.123283	633.953002	8.963379
7.158212	629.512133	8.968397
6.777701	631.538234	8.973415
7.521764	657.140657	8.978432
7.663906	657.872227	8.983450
7.253063	645.627753	8.988467
6.960925	628.793084	8.993485
7.061059	640.594227	8.998503
6.916057	651.296678	9.003520
7.276746	659.316559	9.008538
7.424591	659.693075	9.013555
7.593537	662.514946	9.018573
7.529369	664.184948	9.023591
7.420185	651.207690	9.028608
7.175066	641.204717	9.033626
7.125019	639.643467	9.038643
7.541017	654.681460	9.043661
7.472010	658.585575	9.048679
7.458944	632.220692	9.053696
7.560563	634.442726	9.058714
7.246182	631.551524	9.063731
7.244221	631.062356	9.068749
7.311538	636.182388	9.073767
7.077636	623.523226	9.078784
7.400060	633.756560	9.083802
7.338853	655.795141	9.088819
7.483060	653.718292	9.093837
7.426279	648.656034	9.098855
7.252402	647.341650	9.103872
7.543385	649.127830	9.108890
7.258404	645.029674	9.113907
7.614808	638.829585	9.118925
7.328866	641.924401	9.123943
7.296102	639.031838	9.128960
7.486339	646.877196	9.133978
7.257019	657.549326	9.138995
7.458355	653.357845	9.144013
7.193770	661.057870	9.149031
7.436275	655.673628	9.154048
7.797099	664.764873	9.159066
7.521181	663.186302	9.164083
7.872914	664.702796	9.169101
7.598709	644.914552	9.174119
7.587256	631.720157	9.179136
7.446956	621.913801	9.184154
7.751888	628.058386	9.189171
7.706216	630.701434	9.194189
7.625741	617.564343	9.199207
7.592895	620.532999	9.204224
7.749754	617.449209	9.209242
7.614944	628.322779	9.214259
7.569926	627.425219	9.219277
7.612636	627.129033	9.224295
7.143271	625.163434	9.229312
7.673824	627.878179	9.234330
7.461614	630.470267	9.239347
7.543990	622.652094	9.244365
7.704114	627.687272	9.249383
7.518139	633.230125	9.254400
7.578138	625.538875	9.259418
7.161916	623.675492	9.264435
7.469244	631.606958	9.269453
7.550598	626.930466	9.274471
7.622924	627.647612	9.279488
7.830980	620.604636	9.284506
7.691455	624.282247	9.289523
7.539301	624.150407	9.294541
7.983358	626.631657	9.299559
7.403038	634.721330	9.304576
7.305848	625.878435	9.309594
7.344822	629.648529	9.314611
7.208761	646.878767	9.319629
7.556645	652.951293	9.324647
7.691968	658.278561	9.329664
7.597042	662.575919	9.334682
7.373958	673.359027	9.339699
8.033404	668.158085	9.344717
7.996330	666.697039	9.349735
7.806490	667.898515	9.354752
8.272981	654.873366	9.359770
7.712178	660.475343	9.364787
7.799051	650.305390	9.369805
7.559683	638.916521	9.374823
7.602932	644.494841	9.379840
7.910727	640.247155	9.384858
7.481880	649.863221	9.389875
7.724591	644.804123	9.394893
7.676670	650.856762	9.399911
7.669947	651.208875	9.404928
7.895955	646.283636	9.409946
7.694236	665.482901	9.414963
7.924632	662.513294	9.419981
7.711099	662.966775	9.424999
7.696505	667.916142	9.430016
8.216854	659.963422	9.435034
7.646637	666.445838	9.440051
7.733578	659.360109	9.445069
7.960820	662.443371	9.450087
7.949285	673.911086	9.455104
8.092483	666.671362	9.460122
8.054906	660.873292	9.465139
8.187923	649.938268	9.470157
8.132228	640.045652	9.475175
7.723633	633.952163	9.480192
7.724295	628.533376	9.485210
7.679553	629.768495	9.490227
7.840418	622.526457	9.495245
7.740185	635.183748	9.500263
7.564970	653.421785	9.505280
7.881352	657.833305	9.510298
8.010874	664.941139	9.515315
8.171255	663.213949	9.520333
8.518204	656.365462	9.525351
7.712939	646.461539	9.530368
7.785210	640.251612	9.535386
7.794123	654.515537	9.540403
7.565437	664.544303	9.545421
8.220425	665.781068	9.550439
8.002100	670.944671	9.555456
8.227642	663.857641	9.560474
7.908690	671.396016	9.565491
7.888133	673.589471	9.570509
8.054452	668.602066	9.575527
8.249878	672.729309	9.580544
8.293463	661.227629	9.585562
8.049923	652.334746	9.590579
7.885325	642.058811	9.595597
7.941455	641.504711	9.600615
7.722862	658.866338	9.605632
8.314823	667.646692	9.610650
7.982955	665.755557	9.615667
7.864785	667.031182	9.620685
8.254039	665.871170	9.625703
7.743720	673.375688	9.630720
7.773035	663.100697	9.635738
7.965465	668.899386	9.640755
8.245888	667.884945	9.645773
8.145197	663.708043	9.650791
8.011996	666.407124	9.655808
8.089446	662.229266	9.660826
8.092238	666.648427	9.665843
7.707419	671.375064	9.670861
7.906550	666.065319	9.675879
7.805888	672.360149	9.680896
7.917509	662.934071	9.685914
7.966342	669.930474	9.690931
8.017532	689.925825	9.695949
8.675450	695.329551	9.700967
8.456424	690.401224	9.705984
8.433280	664.647364	9.711002
8.472603	665.658343	9.716019
7.977881	668.330680	9.721037
7.969443	663.314148	9.726055
7.948116	661.893800	9.731072
7.909573	660.109398	9.736090
8.026332	662.337590	9.741107
7.840583	686.976192	9.746125
8.254079	673.303941	9.751143
8.301847	686.057821	9.756160
8.341253	693.634301	9.761178
8.287301	693.846804	9.766195
8.186698	695.591933	9.771213
8.529950	688.608423	9.776231
8.393015	698.239957	9.781248
8.650421	691.630677	9.786266
8.463084	677.247534	9.791283
8.430474	666.793044	9.796301
8.462085	657.182003	9.801319
8.117795	662.321386	9.806336
8.134745	664.407848	9.811354
8.188973	676.294961	9.816371
8.099747	688.844771	9.821389
8.547858	687.735637	9.826407
8.734242	685.488424	9.831424
8.272866	683.841355	9.836442
8.231139	680.188705	9.841459
8.264394	687.206591	9.846477
8.398020	686.822126	9.851495
8.509797	696.279215	9.856512
8.391819	702.043298	9.861530
8.403398	688.368103	9.866547
8.288769	688.739857	9.871565
8.323439	689.151648	9.876583
8.268438	695.733789	9.881600
8.482816	693.772078	9.886618
8.756121	693.665448	9.891635
8.431544	691.561305	9.896653
8.551030	686.788132	9.901671
8.368502	692.843197	9.906688
8.266449	699.335106	9.911706
8.471339	700.595228	9.916723
8.396189	700.102627	9.921741
8.716800	687.273840	9.926759
8.354846	693.682610	9.931776
8.671478	691.342967	9.936794
8.691226	696.201229	9.941811
8.456362	694.876863	9.946829
8.577375	692.251917	9.951847
8.585678	703.296908	9.956864
8.615045	691.350936	9.961882
8.624849	695.660880	9.966899
8.153235	697.416464	9.971917
8.654419	694.924222	9.976935
8.359034	697.025795	9.981952
8.680736	700.708345	9.986970
8.582807	696.808517	9.991987
8.395675	695.180204	9.997005
8.597114	684.142297	10.002023
8.438010	688.804794	10.007040
8.361559	694.106515	10.012058
8.534867	690.639304	10.017075
8.496472	695.322166	10.022093
8.919963	688.497996	10.027111
8.555407	690.562995	10.032128
8.373302	700.438804	10.037146
8.503572	694.622966	10.042163
8.532852	701.289572	10.047181
8.484543	690.721335	10.052199
8.501722	703.296645	10.057216
8.429749	710.417591	10.062234
8.738877	723.909669	10.067251
8.778532	724.417677	10.072269
8.913153	716.152644	10.077287
8.594653	727.466123	10.082304
8.798720	727.743376	10.087322
9.075327	729.326643	10.092339
8.660018	720.975122	10.097357
8.680574	706.446314	10.102375
8.744194	718.761797	10.107392
8.847292	718.425494	10.112410
8.909729	719.150187	10.117427
8.343973	708.354453	10.122445
8.845272	719.707756	10.127463
9.058960	715.924619	10.132480
8.920264	721.213037	10.137498
8.919757	733.497421	10.142515
8.986599	718.944402	10.147533
9.045956	699.160300	10.152551
8.623003	694.743858	10.157568
8.888979	695.226199	10.162586
9.111488	687.956010	10.167603
8.479332	692.043734	10.172621
8.783843	697.236116	10.177639
9.009523	712.248007	10.182656
8.906308	710.939239	10.187674
8.825209	703.844900	10.192691
9.033891	710.515068	10.197709
8.824949	704.647332	10.202727
9.387097	707.618261	10.207744
8.668008	696.516254	10.212762
8.856515	692.008797	10.217779
8.886477	695.411329	10.222797
9.396536	703.693883	10.227815
8.812037	706.634620	10.232832
8.922276	690.060793	10.237850
8.985862	683.308819	10.242867
8.751438	695.656315	10.247885
9.200860	696.387198	10.252903
8.986807	699.219350	10.257920
8.879367	696.664908	10.262938
8.995596	703.200786	10.267955
9.007768	712.526947	10.272973
8.925544	710.642693	10.277991
9.436259	719.842607	10.283008
9.164639	706.649499	10.288026
9.110180	694.244602	10.293043
8.862163	692.134474	10.298061
8.959297	690.954923	10.303079
8.957409	694.816636	10.308096
9.166632	707.995737	10.313114
9.093219	709.651528	10.318131
9.085188	712.622785	10.323149
9.216638	713.623827	10.328167
9.010318	715.892927	10.333184
9.048102	717.005142	10.338202
9.261898	717.202442	10.343219
9.413270	718.610395	10.348237
9.233864	699.858285	10.353255
9.161692	703.456262	10.358272
8.614001	702.253377	10.363290
9.142319	703.262712	10.368307
9.160408	714.139762	10.373325
9.218604	718.422803	10.378343
9.001985	721.956521	10.383360
9.019784	717.977490	10.388378
9.437708	710.666665	10.393395
9.620547	719.208319	10.398413
9.465894	721.267696	10.403431
9.848701	706.619851	10.408448
9.269359	702.062976	10.413466
9.230677	693.796536	10.418483
8.776652	698.217339	10.423501
8.871434	702.834060	10.428519
9.094117	701.672495	10.433536
9.029629	712.431337	10.438554
9.255327	708.934384	10.443571
9.269000	719.172053	10.448589
9.019643	719.410221	10.453607
9.046144	722.322616	10.458624
9.155745	720.419194	10.463642
9.362996	713.642827	10.468659
9.091040	719.759558	10.473677
9.017733	720.616565	10.478695
9.273971	722.789387	10.483712
8.979481	714.930823	10.488730
9.512326	729.476736	10.493747
9.705944	726.787403	10.498765
9.415782	724.159282	10.503783
9.677865	721.938503	10.508800
9.307179	720.542537	10.513818
9.580619	716.729035	10.518835
9.469993	724.417770	10.523853
9.680532	728.274432	10.528871
9.588690	718.655647	10.533888
9.568641	728.364295	10.538906
9.368435	715.633733	10.543923
9.101925	726.563430	10.548941
8.936851	713.820754	10.553959
9.392691	724.585957	10.558976
9.099375	724.826286	10.563994
9.270182	737.258672	10.569011
9.745345	744.877974	10.574029
9.472007	750.539069	10.579047
9.780768	743.558097	10.584064
9.809693	752.676796	10.589082
9.559699	728.383928	10.594099
9.549686	720.975073	10.599117
9.764077	719.314519	10.604135
9.859984	719.358516	10.609152
9.419484	722.086053	10.614170
9.593264	717.904826	10.619187
9.658705	720.451740	10.624205
9.450091	720.140283	10.629223
9.733221	715.029984	10.634240
9.510432	723.767146	10.639258
9.746871	718.337827	10.644275
9.772653	716.921483	10.649293
9.400622	722.342234	10.654311
9.827969	717.964698	10.659328
9.560301	725.232222	10.664346
9.424330	720.334224	10.669363
9.698161	729.950118	10.674381
9.520287	730.226446	10.679399
9.970862	725.388792	10.684416
9.616412	734.126897	10.689434
9.574692	727.277979	10.694451
9.539350	733.388997	10.699469
9.968407	738.530260	10.704487
10.119237	745.222621	10.709504
9.812549	740.545787	10.714522
9.534534	723.339015	10.719539
9.575761	720.190696	10.724557
9.445549	737.478133	10.729575
9.885607	746.663781	10.734592
9.724690	750.565817	10.739610
9.763625	746.746654	10.744627
9.819014	748.909434	10.749645
9.807053	754.011926	10.754663
9.914492	747.098933	10.759680
9.281239	755.075786	10.764698
9.549821	751.929181	10.769715
9.690493	748.201039	10.774733
9.677281	747.231279	10.779751
9.579198	746.430682	10.784768
9.640215	752.493863	10.789786
9.921263	751.175002	10.794803
9.881465	754.797157	10.799821
9.775217	752.346045	10.804839
10.140582	746.918594	10.809856
9.884930	755.098652	10.814874
10.149306	757.689792	10.819891
9.815596	744.564016	10.824909
9.835576	750.663911	10.829927
9.887165	745.836810	10.834944
9.866458	751.124990	10.839962
9.914041	745.676543	10.844979
9.739966	750.393699	10.849997
9.789112	755.960454	10.855015
10.157929	765.059490	10.860032
10.264776	777.527301	10.865050
10.333039	756.678329	10.870067
10.297777	752.790747	10.875085
10.231700	748.109499	10.880103
10.360347	752.084839	10.885120
9.989824	751.713583	10.890138
10.467787	746.489521	10.895155
10.522557	744.810516	10.900173
10.081543	752.456342	10.905191
10.434389	742.734381	10.910208
10.280076	742.684387	10.915226
10.590471	747.888214	10.920243
10.483450	735.136694	10.925261
9.869543	718.578030	10.930279
10.024104	712.605613	10.935296
10.182626	713.378564	10.940314
9.994846	721.652871	10.945331
10.365644	720.102630	10.950349
9.865296	720.774854	10.955367
10.167763	711.859235	10.960384
10.073672	728.910775	10.965402
10.255226	740.994557	10.970419
10.445615	740.648129	10.975437
10.006648	734.040174	10.980455
10.190578	728.821108	10.985472
10.005091	738.081989	10.990490
10.273266	744.158106	10.995507
10.523722	743.622609	11.000525
10.061409	755.178413	11.005543
10.320994	747.502082	11.010560
10.202807	746.251692	11.015578
10.091745	748.545572	11.020595
10.626718	745.215101	11.025613
10.059801	755.927257	11.030631
10.363366	743.755733	11.035648
10.270186	750.821552	11.040666
10.263495	764.828925	11.045683
10.360755	753.582053	11.050701
10.233689	753.993267	11.055719
10.622627	748.541047	11.060736
10.361394	752.111291	11.065754
10.399081	755.919816	11.070771
10.493771	747.292503	11.075789
10.076760	751.392842	11.080807
10.575867	748.868654	11.085824
10.182842	745.306440	11.090842
9.921938	761.762843	11.095859
10.489694	753.693768	11.100877
10.413466	759.294276	11.105895
10.238353	756.023909	11.110912
9.878202	744.399663	11.115930
9.991818	757.126951	11.120947
10.238737	755.894051	11.125965
10.314459	774.731190	11.130983
10.633520	773.817426	11.136000
10.552619	775.981519	11.141018
10.505903	788.809787	11.146035
10.583786	774.737142	11.151053
10.521365	786.186202	11.156071
10.707425	781.563975	11.161088
10.539668	785.312830	11.166106
10.616197	777.113680	11.171123
10.566134	759.641576	11.176141
10.556884	778.799859	11.181159
10.931465	758.455639	11.186176
10.639319	754.687754	11.191194
10.334954	754.776774	11.196211
10.653061	744.472805	11.201229
10.388273	756.296670	11.206247
10.705584	767.594260	11.211264
10.864834	775.232820	11.216282
10.465157	776.013172	11.221299
10.505850	772.718089	11.226317
10.782610	786.501785	11.231335
10.802998	770.633261	11.236352
11.016014	778.388108	11.241370
10.595113	757.151660	11.246387
10.517002	748.714762	11.251405
10.806572	766.990529	11.256423
10.877040	773.712744	11.261440
10.573004	766.928504	11.266458
10.536324	768.693959	11.271475
10.697004	774.484756	11.276493
10.513316	776.558003	11.281511
10.940697	769.901451	11.286528
10.783789	773.143420	11.291546
10.619071	773.242778	11.296563
11.083957	772.539497	11.301581
10.812329	781.022197	11.306599
10.953169	765.567564	11.311616
11.009514	775.524205	11.316634
10.593843	777.912227	11.321651
10.795068	767.840183	11.326669
10.788153	772.307632	11.331687
10.552621	783.462147	11.336704
10.580776	770.165805	11.341722
10.691823	772.764227	11.346739
10.956746	777.396888	11.351757
10.843486	781.744950	11.356775
10.873815	769.297804	11.361792
10.837029	778.553377	11.366810
10.888205	776.264371	11.371827
11.227145	776.461814	11.376845
10.767960	784.867311	11.381863
11.203739	782.697285	11.386880
11.209139	778.701788	11.391898
10.582139	774.010272	11.396915
11.199056	770.169013	11.401933
10.917219	774.363109	11.406951
11.354021	777.971699	11.411968
11.218105	775.538881	11.416986
11.193946	779.364739	11.422003
11.381288	777.583075	11.427021
11.284257	783.472058	11.432039
10.767589	771.582388	11.437056
10.895509	783.988845	11.442074
10.666513	779.184968	11.447091
11.037231	768.836840	11.452109
10.864172	775.199012	11.457127
10.827794	777.143935	11.462144
11.025957	773.305091	11.467162
11.001975	779.094580	11.472179
11.372034	775.162316	11.477197
10.949317	780.575732	11.482215
11.032071	776.011948	11.487232
11.290549	782.124723	11.492250
11.152550	800.694152	11.497267
11.763005	798.361349	11.502285
11.320566	793.501871	11.507303
11.063843	775.260474	11.512320
11.053505	769.935776	11.517338
11.164452	780.016441	11.522355
11.353195	774.517446	11.527373
11.345399	780.320003	11.532391
11.130898	781.915310	11.537408
11.132257	774.801379	11.542426
11.305431	791.936678	11.547443
11.521762	794.350357	11.552461
11.563065	786.627086	11.557479
11.146854	772.302815	11.562496
11.420047	775.879052	11.567514
10.872508	781.126141	11.572531
11.439029	779.712766	11.577549
11.615904	796.975402	11.582567
11.373324	794.269709	11.587584
11.224141	777.840708	11.592602
11.568472	789.945996	11.597619
11.558293	783.424882	11.602637
11.343651	778.541073	11.607655
11.312586	772.117117	11.612672
11.449376	788.612413	11.617690
11.526239	793.930905	11.622707
11.674006	787.738732	11.627725
11.264267	777.311972	11.632743
11.260571	791.242107	11.637760
11.617247	796.115471	11.642778
11.496270	794.948211	11.647795
11.373060	784.736190	11.652813
11.525155	805.446434	11.657831
11.450332	798.083312	11.662848
11.633817	791.628939	11.667866
11.627707	800.611744	11.672883
11.849995	801.649322	11.677901
11.662077	797.701578	11.682919
11.567425	783.415384	11.687936
11.523913	777.368267	11.692954
11.362096	793.465797	11.697971
11.808689	798.493554	11.702989
11.512131	806.188709	11.708007
11.613484	797.026832	11.713024
11.966427	798.634866	11.718042
11.519809	803.294812	11.723059
11.586221	801.502857	11.728077
12.092961	796.661786	11.733095
11.643081	786.186158	11.738112
11.528148	766.938673	11.743130
11.640990	785.620082	11.748147
12.038250	793.694408	11.753165
11.290777	781.922865	11.758183
11.674248	795.911328	11.763200
11.814257	783.946766	11.768218
11.610885	807.556650	11.773235
11.605082	795.680394	11.778253
11.672131	803.440529	11.783271
11.305774	805.677090	11.788288
11.796607	792.112000	11.793306
11.904247	803.699045	11.798323
12.079936	803.638892	11.803341
11.714979	805.026846	11.808359
11.475538	802.026161	11.813376
12.086722	804.645703	11.818394
11.746605	804.088318	11.823411
11.936329	797.103413	11.828429
11.803575	804.539174	11.833447
11.718458	799.706348	11.838464
11.989336	795.318481	11.843482
11.792093	801.675614	11.848499
12.182156	797.071960	11.853517
11.707628	799.405168	11.858535
11.818593	794.481217	11.863552
12.025185	793.806534	11.868570
11.803031	795.523182	11.873587
11.916565	803.279162	11.878605
12.144886	808.560375	11.883623
11.622259	806.649828	11.888640
12.179039	798.649079	11.893658
12.191479	804.382943	11.898675
11.953578	796.816524	11.903693
12.093783	792.522733	11.908711
11.655688	797.970983	11.913728
11.974935	802.513953	11.918746
12.022077	815.579836	11.923763
12.330134	822.419020	11.928781
12.247919	812.871413	11.933799
12.140611	803.101602	11.938816
12.573952	783.916055	11.943834
12.385706	794.802920	11.948851
11.993605	790.790963	11.953869
12.118020	786.203744	11.958887
11.974118	795.869167	11.963904
12.328822	781.743984	11.968922
12.339699	780.287192	11.973939
12.475672	776.351172	11.978957
12.285340	777.652731	11.983975
12.424126	781.245714	11.988992
12.208859	781.768378	11.994010
12.286793	773.991806	11.999027
12.173982	776.066702	12.004045
12.233991	777.922046	12.009063
11.960046	780.672798	12.014080
12.202916	772.194546	12.019098
12.115745	776.848898	12.024115
11.968847	775.119431	12.029133
12.301791	781.855663	12.034151
12.118887	797.078001	12.039168
12.108437	800.528387	12.044186
12.344420	813.002795	12.049203
12.769152	811.959726	12.054221
12.449333	808.688901	12.059239
12.588896	813.973791	12.064256
12.797080	805.471345	12.069274
12.335342	807.541428	12.074291
12.072459	779.509887	12.079309
12.494821	797.991248	12.084327
12.175187	805.275681	12.089344
12.398051	810.858963	12.094362
12.512935	822.623158	12.099379
12.311317	814.256673	12.104397
12.618519	813.150786	12.109415
12.463198	818.766774	12.114432
12.619166	815.447083	12.119450
12.619681	823.634362	12.124467
12.674756	818.627144	12.129485
12.686450	818.161494	12.134503
12.366218	823.483943	12.139520
12.639416	823.867460	12.144538
12.654566	824.539362	12.149555
12.637399	837.210423	12.154573
12.759242	828.552981	12.159591
12.338625	827.911293	12.164608
12.511986	822.139647	12.169626
12.513047	827.587232	12.174643
12.024119	832.615589	12.179661
12.188297	817.492848	12.184679
12.619693	824.199411	12.189696
12.555327	831.582918	12.194714
12.344443	829.608543	12.199731
12.272317	827.717484	12.204749
12.451721	838.920252	12.209767
12.457041	857.034939	12.214784
12.906281	841.486646	12.219802
13.026311	839.718483	12.224819
12.884818	840.952514	12.229837
13.509490	844.813067	12.234855
12.893339	833.550025	12.239872
12.717286	815.764880	12.244890
13.025625	812.619553	12.249907
12.992467	808.411155	12.254925
12.969091	805.313277	12.259943
12.740873	813.985645	12.264960
13.014802	815.813052	12.269978
13.109959	820.183303	12.274995
12.920298	813.136809	12.280013
13.317827	801.688615	12.285031
12.843864	811.763405	12.290048
13.117961	816.523686	12.295066
12.874216	803.788450	12.300083
12.638087	807.557688	12.305101
13.186475	806.539022	12.310119
13.219000	805.742777	12.315136
12.815237	810.155092	12.320154
12.942992	810.704416	12.325171
12.677034	812.823572	12.330189
13.109123	806.053239	12.335207
13.234567	807.873345	12.340224
13.015393	812.083844	12.345242
13.046224	808.435683	12.350259
13.129731	812.931082	12.355277
13.114399	807.843011	12.360295
12.858682	815.796747	12.365312
13.271335	810.750792	12.370330
13.301336	807.723598	12.375347
13.089706	810.062878	12.380365
13.238907	804.569239	12.385383
13.036045	807.008636	12.390400
13.110643	814.804531	12.395418
13.170923	810.195643	12.400435
13.434255	819.155495	12.405453
13.197090	808.878080	12.410471
13.113956	816.974095	12.415488
13.072989	818.222973	12.420506
12.948463	811.596379	12.425523
12.694280	811.170819	12.430541
13.100817	807.743106	12.435559
12.821919	810.029749	12.440576
13.142270	827.243072	12.445594
13.307649	835.477464	12.450611
12.947442	836.675668	12.455629
13.086803	847.364236	12.460647
13.219067	844.270105	12.465664
13.417523	850.507406	12.470682
13.598290	843.075563	12.475699
13.389114	848.389079	12.480717
13.388137	833.661366	12.485735
13.337732	852.078959	12.490752
13.240398	843.448353	12.495770
13.393535	839.002023	12.500787
13.120493	848.667210	12.505805
13.556491	841.073032	12.510823
12.993266	847.132538	12.515840
13.163798	844.372208	12.520858
13.487460	839.681511	12.525875
13.125162	852.332968	12.530893
13.513885	846.259918	12.535911
13.263468	853.192380	12.540928
13.433804	861.883419	12.545946
13.645531	866.179659	12.550963
13.864259	869.746828	12.555981
13.863363	852.028695	12.560999
13.743696	843.137629	12.566016
13.413975	837.657931	12.571034
13.440184	829.223005	12.576051
13.388495	845.123623	12.581069
13.769484	840.573424	12.586087
13.414290	848.833397	12.591104
13.474624	861.031434	12.596122
13.517509	864.932820	12.601139
13.720637	870.147758	12.606157
13.986998	855.081678	12.611175
13.877309	868.675910	12.616192
13.687801	864.902419	12.621210
14.151164	855.684106	12.626227
13.656213	850.391992	12.631245
13.777923	835.882924	12.636263
13.486567	838.240528	12.641280
13.918396	857.360514	12.646298
13.993505	854.503391	12.651315
13.915597	842.571326	12.656333
14.127207	836.209910	12.661351
13.879391	835.058139	12.666368
13.692099	826.333783	12.671386
14.039415	832.330691	12.676403
13.559787	829.317808	12.681421
13.702550	830.710269	12.686439
13.952692	832.888054	12.691456
14.096540	832.637121	12.696474
13.873236	830.037673	12.701491
13.818785	830.047910	12.706509
13.884526	826.724260	12.711527
13.862951	833.009405	12.716544
14.289986	854.295414	12.721562
13.806939	834.790707	12.726579
14.096179	844.970624	12.731597
14.198141	849.547619	12.736615
14.095297	833.649438	12.741632
14.115240	833.750894	12.746650
14.241449	828.359080	12.751667
14.005403	835.823770	12.756685
13.811017	833.705332	12.761703
14.260050	825.485023	12.766720
13.728807	841.083177	12.771738
13.887896	840.047481	12.776755
13.901291	858.992676	12.781773
14.065273	864.247557	12.786791
14.268598	864.065117	12.791808
14.126661	868.838795	12.796826
14.308973	860.661453	12.801843
14.085621	866.738698	12.806861
14.323117	869.276043	12.811879
14.496251	862.574943	12.816896
14.230371	865.529086	12.821914
14.395834	859.617010	12.826931
14.410693	854.037731	12.831949
14.456112	838.166566	12.836967
14.083246	832.408598	12.841984
14.058143	833.521787	12.847002
14.481613	841.728011	12.852019
14.276825	834.018302	12.857037
14.109064	832.986339	12.862055
14.102339	838.758426	12.867072
14.173050	860.410515	12.872090
14.123614	855.051713	12.877107
14.264790	862.036259	12.882125
14.118114	861.563370	12.887143
14.262834	856.167693	12.892160
14.450404	869.339889	12.897178
14.465504	860.846946	12.902195
14.042444	865.812835	12.907213
14.153883	864.952735	12.912231
14.548656	860.870696	12.917248
14.350958	864.088337	12.922266
14.304130	857.965364	12.927283
14.605731	853.241704	12.932301
14.601007	858.851273	12.937319
14.367466	859.331692	12.942336
14.476809	860.054924	12.947354
14.884763	869.463666	12.952371
14.672555	865.984469	12.957389
14.689041	864.951520	12.962407
14.713421	859.924963	12.967424
14.308198	866.862987	12.972442
14.629375	859.566932	12.977459
14.827281	867.597147	12.982477
14.598092	866.264346	12.987495
14.509334	859.617242	12.992512
14.651075	868.614972	12.997530
14.775518	872.589859	13.002547
14.789067	882.062737	13.007565
14.755963	875.540262	13.012583
14.986763	864.961316	13.017600
14.665165	863.743024	13.022618
14.668732	857.425890	13.027635
15.164042	865.774160	13.032653
14.507357	867.796221	13.037671
14.827519	855.664772	13.042688
14.860357	868.415370	13.047706
15.239432	866.131500	13.052723
14.777811	868.014967	13.057741
14.887005	860.041060	13.062759
15.116607	854.783683	13.067776
14.645823	856.211604	13.072794
15.092394	859.372559	13.077811
15.065785	854.483179	13.082829
14.930978	861.837816	13.087847
15.033175	847.256382	13.092864
14.679433	865.422268	13.097882
15.047516	852.067206	13.102899
15.050354	857.372782	13.107917
14.676388	858.379576	13.112935
15.123950	865.775962	13.117952
14.959925	869.598626	13.122970
15.191493	864.867662	13.127987
15.114677	868.169613	13.133005
14.582976	855.775308	13.138023
15.034543	870.807623	13.143040
15.090341	880.001471	13.148058
15.277346	872.680779	13.153075
15.293473	883.981873	13.158093
15.225528	881.490935	13.163111
15.448820	878.783277	13.168128
15.052359	873.400046	13.173146
15.200923	863.456733	13.178163
15.191014	862.899782	13.183181
15.107656	869.740419	13.188199
15.027139	871.319061	13.193216
15.184080	882.462198	13.198234
15.288581	876.183064	13.203251
14.975258	884.094408	13.208269
15.090971	884.090641	13.213287
15.224183	872.868042	13.218304
14.930860	890.312967	13.223322
15.401542	880.845015	13.228339
15.465775	874.072971	13.233357
15.391203	871.425266	13.238375
15.940698	881.171583	13.243392
15.289312	879.302031	13.248410
15.516364	871.216875	13.253427
15.725310	886.739750	13.258445
15.506292	884.017936	13.263463
15.662265	877.507062	13.268480
15.663342	880.063085	13.273498
15.450272	863.866213	13.278515
15.306501	859.626907	13.283533
15.438621	874.916442	13.288551
15.813195	867.663507	13.293568
15.523013	869.193013	13.298586
15.596274	862.445068	13.303603
15.275547	856.398944	13.308621
15.278750	865.612910	13.313639
15.687845	872.976695	13.318656
15.856686	877.882370	13.323674
15.536557	871.567652	13.328691
16.036738	866.165471	13.333709
15.640431	869.150661	13.338727
15.661664	856.781718	13.343744
15.492743	866.428888	13.348762
15.579579	871.298930	13.353779
15.802542	869.409000	13.358797
15.586816	878.268301	13.363815
15.891438	867.059447	13.368832
15.806258	872.198904	13.373850
15.940046	872.533464	13.378867
15.851498	868.753096	13.383885
15.642994	872.406363	13.388903
15.825996	862.867167	13.393920
15.909435	870.334874	13.398938
15.995722	869.662787	13.403955
15.806895	862.624400	13.408973
15.918653	872.436109	13.413991
16.016163	861.771762	13.419008
16.101394	876.402563	13.424026
15.964021	852.271156	13.429043
15.809087	841.680906	13.434061
15.627908	849.822699	13.439079
16.053168	851.179014	13.444096
15.947933	872.045339	13.449114
15.714992	868.429030	13.454131
15.683877	875.463764	13.459149
15.828625	876.082714	13.464167
15.978401	872.906154	13.469184
15.876300	877.870472	13.474202
15.815795	877.172300	13.479219
15.791700	869.428323	13.484237
15.618644	870.361300	13.489255
15.933178	867.079905	13.494272
15.548850	870.080039	13.499290
16.155611	889.302194	13.504307
16.379842	896.963911	13.509325
16.287227	900.620435	13.514343
16.387723	885.750285	13.519360
16.302048	880.484872	13.524378
16.230835	873.704155	13.529395
16.459360	872.310522	13.534413
16.419351	867.327299	13.539431
16.397091	858.395292	13.544448
15.970187	862.805155	13.549466
16.335220	859.812626	13.554483
16.498821	856.085385	13.559501
16.343529	858.784221	13.564519
16.189429	852.348323	13.569536
16.083058	858.362890	13.574554
16.600752	849.373760	13.579571
16.478098	854.565084	13.584589
16.055119	869.281213	13.589607
16.294761	858.053993	13.594624
16.487316	861.766824	13.599642
16.245559	860.670738	13.604659
16.424750	860.411197	13.609677
16.511820	875.761733	13.614695
16.617233	877.342657	13.619712
16.607537	874.551145	13.624730
16.526549	866.008760	13.629747
16.481011	862.073248	13.634765
16.318292	863.276939	13.639783
16.486513	873.902483	13.644800
16.553518	887.787535	13.649818
16.402022	896.525586	13.654835
16.450427	889.515224	13.659853
16.385316	884.640871	13.664871
16.568556	892.270006	13.669888
16.842016	891.948794	13.674906
16.760713	887.707010	13.679923
16.942197	890.346935	13.684941
16.852989	892.665956	13.689959
17.122768	884.855593	13.694976
16.978237	888.139628	13.699994
16.523583	871.174921	13.705011
16.598060	871.187823	13.710029
17.152794	883.200868	13.715047
16.674360	870.078477	13.720064
16.313435	872.671609	13.725082
16.638114	878.239631	13.730099
16.565928	882.492342	13.735117
16.450986	885.879739	13.740135
16.467577	886.917528	13.745152
16.502900	882.200945	13.750170
16.430693	889.672782	13.755187
16.774055	894.021638	13.760205
16.608512	908.108592	13.765223
17.120557	905.768842	13.770240
17.274575	909.551449	13.775258
17.164104	920.503473	13.780275
17.398433	904.583244	13.785293
17.311603	896.604772	13.790311
17.337839	886.217944	13.795328
17.251659	886.816082	13.800346
17.071692	883.876788	13.805363
17.252857	881.903626	13.810381
16.918590	888.082312	13.815399
17.036214	884.865801	13.820416
17.086249	886.220081	13.825434
16.803985	890.409160	13.830451
17.025003	881.908879	13.835469
16.654039	882.503782	13.840487
17.050981	898.088840	13.845504
17.125936	911.400580	13.850522
17.188595	919.123706	13.855539
17.417536	908.497797	13.860557
17.218013	918.618546	13.865575
17.344543	912.423541	13.870592
17.595589	910.372271	13.875610
17.152438	904.976289	13.880627
17.013535	896.545834	13.885645
17.188482	902.718549	13.890663
17.241684	901.186630	13.895680
17.326824	904.166116	13.900698
17.435673	905.640968	13.905715
17.243638	908.558090	13.910733
16.973123	907.374247	13.915751
17.549408	916.055181	13.920768
17.213463	911.072131	13.925786
17.214509	908.256789	13.930803
17.224527	910.649928	13.935821
17.176829	908.393022	13.940839
17.723252	904.956298	13.945856
17.389620	901.568455	13.950874
16.968328	912.766813	13.955891
17.686463	922.908438	13.960909
17.481057	934.294674	13.965927
17.869067	928.998444	13.970944
17.797046	915.791002	13.975962
17.832005	917.999706	13.980979
17.638704	900.845240	13.985997
17.647757	910.119284	13.991015
17.582042	896.599806	13.996032
17.537059	904.569871	14.001050
17.363771	910.950245	14.006067
17.760253	928.192018	14.011085
18.126488	935.175155	14.016103
18.353931	915.029495	14.021120
18.289329	911.296330	14.026138
18.053048	905.086212	14.031155
18.191966	905.936038	14.036173
18.220417	906.214423	14.041191
17.803417	895.291566	14.046208
18.132099	900.854603	14.051226
17.615588	894.431062	14.056243
18.093055	897.002688	14.061261
18.257347	904.341280	14.066279
18.377533	888.958838	14.071296
17.967053	878.673463	14.076314
17.890812	870.584988	14.081331
17.836941	864.615533	14.086349
17.864103	874.176698	14.091367
18.016802	881.234538	14.096384
18.068500	891.860885	14.101402
17.712451	903.316136	14.106419
18.323213	903.740604	14.111437
18.212706	901.998798	14.116455
18.120551	896.989950	14.121472
18.408195	902.587341	14.126490
17.827218	888.035533	14.131507
18.339886	892.724052	14.136525
18.154645	890.126557	14.141543
18.260916	887.541419	14.146560
18.341823	889.923604	14.151578
17.629089	880.925612	14.156595
18.214640	880.668858	14.161613
18.024684	894.457497	14.166631
17.974192	898.982196	14.171648
18.150424	899.066040	14.176666
17.909196	905.133270	14.181683
18.107775	901.632497	14.186701
18.221753	900.753866	14.191719
17.886722	898.845706	14.196736
17.589049	905.665156	14.201754
18.275815	922.548636	14.206771
18.262821	930.489796	14.211789
18.371662	932.933501	14.216807
18.177767	928.470203	14.221824
18.548945	925.734506	14.226842
18.269372	940.182874	14.231859
18.511735	937.586610	14.236877
18.297955	934.250957	14.241895
18.375731	934.367245	14.246912
18.426530	931.058645	14.251930
18.258220	933.401793	14.256947
18.495239	930.616266	14.261965
18.166744	934.101237	14.266983
18.499852	940.607209	14.272000
18.612692	947.827971	14.277018
19.053680	945.761779	14.282035
18.925513	932.533700	14.287053
18.791333	928.736071	14.292071
18.696192	924.108005	14.297088
18.737422	920.002214	14.302106
18.506880	921.030929	14.307123
18.866314	923.024103	14.312141
18.841786	913.384601	14.317159
18.557416	917.255155	14.322176
19.033404	912.829750	14.327194
18.709779	914.351019	14.332211
19.153572	915.683800	14.337229
18.700870	912.323938	14.342247
18.590007	918.131802	14.347264
18.764475	919.933961	14.352282
19.442677	936.414958	14.357299
19.141942	925.561799	14.362317
18.978633	921.920169	14.367335
18.564788	925.973180	14.372352
18.769738	917.282242	14.377370
18.874724	932.260202	14.382387
18.799063	930.941341	14.387405
18.792181	944.600108	14.392423
18.989481	944.950529	14.397440
19.374393	943.398323	14.402458
19.076276	953.117725	14.407475
18.957495	947.658174	14.412493
19.021010	948.985426	14.417511
19.325523	953.884800	14.422528
19.357285	946.279166	14.427546
18.905188	946.144235	14.432563
19.438350	942.731744	14.437581
19.383755	935.308516	14.442599
19.136705	950.193218	14.447616
19.617233	933.790875	14.452634
19.097677	949.820645	14.457651
18.669719	946.575964	14.462669
19.033815	950.110420	14.467687
18.936885	943.730761	14.472704
19.077927	937.221154	14.477722
19.103168	951.605280	14.482739
19.428255	940.628012	14.487757
19.356356	943.807911	14.492775
18.935471	952.151646	14.497792
18.924815	964.836301	14.502810
19.236508	974.472061	14.507827
19.553129	979.191494	14.512845
19.539939	970.221309	14.517863
19.550467	969.292484	14.522880
19.967255	970.433687	14.527898
19.959136	965.253430	14.532915
19.794471	952.829370	14.537933
20.026241	940.471165	14.542951
19.561834	935.721573	14.547968
19.580540	938.336889	14.552986
19.632057	928.842652	14.558003
19.810559	938.555954	14.563021
19.847249	925.396247	14.568039
19.782155	931.966972	14.573056
19.510061	926.158031	14.578074
19.471235	929.259619	14.583091
19.289793	936.519656	14.588109
19.524902	941.411622	14.593127
19.404851	950.624001	14.598144
19.901691	949.025703	14.603162
19.803678	965.956507	14.608179
20.024505	963.487026	14.613197
20.232998	960.904240	14.618215
20.318770	961.016843	14.623232
20.437766	942.976011	14.628250
20.087187	934.981746	14.633267
19.837467	922.996970	14.638285
20.099333	923.679202	14.643303
19.847989	930.089437	14.648320
20.222389	927.257542	14.653338
20.153333	931.864455	14.658355
19.468573	924.768402	14.663373
19.711029	922.352431	14.668391
19.525072	942.507844	14.673408
19.966627	945.003145	14.678426
20.253358	950.715660	14.683443
20.204473	970.014201	14.688461
20.339868	960.908398	14.693479
20.087529	964.682326	14.698496
20.147309	950.318045	14.703514
19.989172	960.509130	14.708531
20.222676	968.470907	14.713549
20.294241	957.284438	14.718567
20.033512	962.617159	14.723584
20.420717	952.812610	14.728602
20.404281	958.320616	14.733619
20.291225	964.263500	14.738637
20.393507	967.724389	14.743655
20.102508	957.095570	14.748672
20.052822	961.991002	14.753690
20.374217	965.216405	14.758707
20.273034	963.367147	14.763725
20.275287	963.504997	14.768743
20.265444	970.176819	14.773760
20.478226	960.138955	14.778778
20.436782	966.889234	14.783795
20.190190	963.868048	14.788813
20.440044	956.618796	14.793831
20.408554	968.682525	14.798848
20.732136	962.221023	14.803866
20.569675	960.479152	14.808883
20.180334	959.904716	14.813901
20.758843	970.330898	14.818919
20.784985	984.624359	14.823936
21.097335	977.335223	14.828954
21.073670	963.839431	14.833971
21.004767	960.247116	14.838989
20.942395	953.451121	14.844007
20.648221	950.181137	14.849024
20.617723	947.038350	14.854042
20.604999	949.790755	14.859059
20.544312	950.640173	14.864077
20.893895	950.993723	14.869095
20.582644	957.982760	14.874112
20.351244	948.196399	14.879130
20.503802	963.119663	14.884147
20.531913	973.475576	14.889165
20.629074	983.738570	14.894183
20.752522	986.041288	14.899200
21.261860	979.854912	14.904218
21.145887	975.874738	14.909235
20.779544	979.015215	14.914253
20.866550	968.015148	14.919271
20.807178	977.389535	14.924288
21.212359	974.450965	14.929306
21.233147	965.308234	14.934323
21.286440	976.069409	14.939341
21.223833	974.092508	14.944359
21.009234	977.091328	14.949376
21.074792	966.083004	14.954394
21.603946	964.928151	14.959411
21.493376	969.971063	14.964429
21.207137	972.523498	14.969447
21.374043	975.270179	14.974464
21.142605	970.320983	14.979482
21.422106	970.099946	14.984499
21.423881	986.895751	14.989517
21.604399	969.972995	14.994535
21.376886	971.505518	14.999552
21.589970	974.396513	15.004570
21.510371	968.844644	15.009587
21.126328	972.032143	15.014605
21.248628	963.965072	15.019623
21.318485	964.289355	15.024640
21.224093	969.997272	15.029658
21.692911	963.699507	15.034675
21.431654	966.961551	15.039693
21.718386	965.663384	15.044711
21.299533	974.107971	15.049728
21.480090	972.742350	15.054746
21.627749	970.870389	15.059763
21.617929	968.265486	15.064781
21.517023	964.403287	15.069799
21.636499	966.988930	15.074816
21.329981	966.804697	15.079834
21.553661	961.926986	15.084851
21.235216	968.660537	15.089869
21.664675	965.269545	15.094887
21.500911	981.434912	15.099904
21.325010	991.131344	15.104922
21.859962	1003.502073	15.109939
21.843143	1007.359841	15.114957
22.002868	1002.503337	15.119975
22.023495	1006.988340	15.124992
21.637877	1005.230662	15.130010
21.794600	1001.097851	15.135027
21.644233	1005.887927	15.140045
21.992714	999.947066	15.145063
21.981545	1009.902440	15.150080
22.080226	1001.292042	15.155098
22.141850	999.432749	15.160115
22.085385	1002.807733	15.165133
22.302459	993.919478	15.170151
22.424584	1003.646881	15.175168
22.148963	987.877933	15.180186
22.315346	970.702804	15.185203
21.993925	973.657503	15.190221
22.255483	964.611906	15.195239
22.049183	969.056919	15.200256
22.323528	977.924888	15.205274
22.423109	964.446480	15.210291
22.073445	966.212999	15.215309
21.997420	961.938038	15.220327
22.258130	979.353525	15.225344
22.023045	987.895243	15.230362
22.386510	997.176793	15.235379
22.612960	1001.491105	15.240397
22.245386	991.193824	15.245415
22.507230	990.958389	15.250432
22.079202	990.036437	15.255450
21.969793	993.000126	15.260467
22.054102	997.243096	15.265485
22.229204	989.802673	15.270503
22.262897	999.030960	15.275520
22.104660	999.171763	15.280538
22.474823	995.755544	15.285555
22.169940	998.191786	15.290573
22.489928	996.223180	15.295591
22.207758	1003.443630	15.300608
22.356302	998.320094	15.305626
22.402250	1010.013174	15.310643
22.331489	1016.883285	15.315661
22.532898	1015.157136	15.320679
22.526411	1023.757080	15.325696
22.531710	1018.004135	15.330714
22.683088	1020.058544	15.335731
22.315331	1013.225299	15.340749
22.788358	1014.577263	15.345767
22.783822	1013.846197	15.350784
22.689173	1016.754693	15.355802
23.119528	1015.198499	15.360819
22.805514	1017.125254	15.365837
22.891444	1001.702705	15.370855
23.129314	1013.572661	15.375872
22.871054	1019.301431	15.380890
22.899965	1004.223346	15.385907
22.846522	1021.504688	15.390925
23.113254	1018.007171	15.395943
23.158944	1014.475393	15.400960
22.812358	1022.411999	15.405978
23.315996	1030.605838	15.410995
22.992415	1027.587545	15.416013
23.015900	1034.434578	15.421031
23.187476	1030.108363	15.426048
23.531371	1039.726235	15.431066
23.482536	1017.517620	15.436083
23.297148	1017.683784	15.441101
23.398960	1014.210427	15.446119
22.935149	1002.487800	15.451136
23.095911	1012.314711	15.456154
23.269044	1006.585552	15.461171
23.419638	1012.697780	15.466189
23.375713	1006.952203	15.471207
23.330100	1007.588114	15.476224
23.344300	1011.932063	15.481242
23.741083	1009.297225	15.486259
23.356147	1010.644018	15.491277
23.386707	1010.914182	15.496295
23.476404	1009.543525	15.501312
23.166603	1005.405289	15.506330
23.642201	1017.523665	15.511347
23.874982	1022.446357	15.516365
23.601067	1011.099348	15.521383
23.635769	1008.600053	15.526400
23.464526	1007.731639	15.531418
23.912582	994.338410	15.536435
23.461910	1007.004232	15.541453
23.111470	1009.942484	15.546471
24.019259	1017.683585	15.551488
23.831556	1025.180123	15.556506
23.786645	1019.653198	15.561523
23.600332	1017.714885	15.566541
23.741447	1017.156149	15.571559
24.048780	1026.400162	15.576576
23.598285	1023.182030	15.581594
23.917502	1026.211753	15.586611
24.095807	1030.175793	15.591629
23.810486	1021.769120	15.596647
23.679047	1025.285651	15.601664
23.779610	1033.265539	15.606682
23.826745	1034.237652	15.611699
24.011974	1044.600666	15.616717
23.940282	1037.583352	15.621735
24.180221	1038.352288	15.626752
23.747542	1044.470563	15.631770
24.141608	1035.757693	15.636787
23.761949	1036.117043	15.641805
23.875691	1037.195839	15.646823
24.133636	1032.991142	15.651840
23.982623	1039.713141	15.656858
24.011917	1035.210494	15.661875
23.975243	1036.962200	15.666893
23.944950	1028.728245	15.671911
24.047970	1027.567575	15.676928
23.820989	1044.222588	15.681946
24.195997	1049.405584	15.686963
24.172293	1051.902750	15.691981
24.412333	1058.256867	15.696999
24.538759	1058.921377	15.702016
24.656432	1065.517010	15.707034
24.766915	1054.005929	15.712051
24.359616	1057.042972	15.717069
24.596183	1064.196846	15.722087
24.676321	1051.496353	15.727104
24.304833	1050.309928	15.732122
24.802136	1045.162876	15.737139
24.481958	1049.731882	15.742157
24.662969	1050.233816	15.747175
24.888750	1047.598549	15.752192
24.394104	1051.039013	15.757210
24.592460	1041.512913	15.762227
25.022688	1053.862050	15.767245
24.322019	1041.199915	15.772263
24.843769	1045.224014	15.777280
24.805557	1058.230224	15.782298
24.917617	1050.385267	15.787315
24.315963	1054.380042	15.792333
24.851920	1055.043272	15.797351
25.111927	1046.762025	15.802368
24.993551	1052.473944	15.807386
25.210061	1045.083328	15.812403
25.131083	1047.192419	15.817421
25.004366	1032.716429	15.822439
24.544591	1025.388988	15.827456
24.850818	1042.367501	15.832474
25.155483	1042.590703	15.837491
24.997620	1058.414243	15.842509
25.077953	1046.055047	15.847527
25.337251	1052.871308	15.852544
25.130433	1054.909052	15.857562
25.280912	1052.593720	15.862579
25.339612	1064.407166	15.867597
24.766153	1036.833652	15.872615
25.062411	1048.838055	15.877632
25.116614	1049.299572	15.882650
25.371110	1051.600285	15.887667
25.365419	1053.575199	15.892685
25.132770	1054.594823	15.897703
25.440917	1047.630352	15.902720
25.261662	1051.249291	15.907738
25.325712	1052.087901	15.912755
25.299740	1049.735649	15.917773
25.308689	1056.617380	15.922791
25.305792	1047.984801	15.927808
25.231160	1055.301219	15.932826
25.118927	1050.113371	15.937843
24.884980	1054.056314	15.942861
25.505209	1053.561150	15.947879
25.558925	1050.616986	15.952896
25.320942	1057.169937	15.957914
25.474946	1068.635335	15.962931
25.869321	1079.536159	15.967949
25.813092	1082.233589	15.972967
25.671349	1050.687148	15.977984
25.600047	1059.012423	15.983002
25.702798	1071.964989	15.988019
26.010919	1079.383388	15.993037
25.749288	1068.861435	15.998055
25.914312	1051.201029	16.003072
25.249794	1063.433822	16.008090
25.817527	1067.586527	16.013107
25.747430	1064.206976	16.018125
25.894566	1076.516790	16.023143
26.295889	1070.837614	16.028160
25.743921	1080.492834	16.033178
25.908780	1067.544058	16.038195
26.316171	1074.024008	16.043213
26.190424	1081.661095	16.048231
26.363074	1069.019676	16.053248
26.196029	1070.390234	16.058266
25.935512	1065.827303	16.063283
26.020995	1067.019043	16.068301
25.844730	1061.007182	16.073319
26.161177	1060.591059	16.078336
26.098778	1069.131392	16.083354
25.775824	1072.485559	16.088371
26.119073	1067.153389	16.093389
26.176245	1072.041004	16.098407
26.423267	1062.083622	16.103424
26.122236	1061.221341	16.108442
26.236128	1059.205755	16.113459
26.127899	1065.478180	16.118477
25.879057	1067.766575	16.123495
26.434843	1079.187892	16.128512
26.373264	1093.816046	16.133530
26.325949	1088.424135	16.138547
26.518120	1099.747022	16.143565
26.622043	1096.582734	16.148583
26.880609	1090.489018	16.153600
26.732245	1098.292056	16.158618
26.851899	1089.460428	16.163635
26.861966	1096.560881	16.168653
26.447343	1090.608555	16.173671
26.799949	1087.357423	16.178688
26.818118	1086.643853	16.183706
27.035902	1084.975219	16.188723
26.816673	1073.624620	16.193741
26.949744	1067.729639	16.198759
26.771279	1055.169992	16.203776
26.686865	1058.183489	16.208794
26.836266	1071.525952	16.213811
27.387394	1072.481147	16.218829
26.740227	1068.296398	16.223847
26.971493	1054.803587	16.228864
26.923976	1060.554955	16.233882
26.972707	1064.527074	16.238899
27.126260	1058.512962	16.243917
26.896879	1064.456642	16.248935
27.127719	1069.777292	16.253952
27.061371	1075.376277	16.258970
27.139184	1082.452908	16.263987
27.354914	1077.523330	16.269005
27.067113	1072.866493	16.274023
27.008254	1069.986634	16.279040
26.982752	1079.668060	16.284058
26.745073	1081.294793	16.289075
27.358869	1078.127968	16.294093
27.235299	1095.532417	16.299111
27.240614	1085.931172	16.304128
27.403585	1084.768051	16.309146
27.439212	1084.375199	16.314163
27.324872	1075.365011	16.319181
27.157059	1078.215951	16.324199
27.273640	1076.590847	16.329216
27.499103	1077.628312	16.334234
27.197284	1073.495035	16.339251
27.356920	1075.792168	16.344269
27.365078	1079.730067	16.349287
27.564685	1093.492171	16.354304
27.671179	1104.919009	16.359322
27.925974	1108.045632	16.364339
27.916408	1098.362989	16.369357
27.373016	1084.498837	16.374375
27.446972	1098.057350	16.379392
27.756552	1102.633112	16.384410
27.572932	1109.036931	16.389427
27.849796	1110.914674	16.394445
27.843298	1107.419468	16.399463
27.917013	1105.090856	16.404480
28.015095	1103.129061	16.409498
27.660404	1111.539477	16.414515
28.050340	1096.028702	16.419533
27.908819	1101.430310	16.424551
27.945362	1095.824519	16.429568
27.924392	1094.496981	16.434586
27.912706	1101.412857	16.439603
28.211282	1100.033982	16.444621
27.752253	1102.079638	16.449639
27.983372	1093.592921	16.454656
27.972594	1097.858357	16.459674
28.197330	1102.548163	16.464691
28.036551	1104.302317	16.469709
28.058755	1100.981094	16.474727
28.427711	1109.931894	16.479744
28.529020	1113.598087	16.484762
28.301080	1105.565316	16.489779
28.471918	1095.671707	16.494797
28.617587	1097.460546	16.499815
28.328085	1094.103540	16.504832
28.452593	1097.358818	16.509850
28.268707	1099.703388	16.514867
28.576294	1095.508565	16.519885
28.087565	1108.770905	16.524903
28.539087	1121.057517	16.529920
28.770134	1127.341501	16.534938
28.612094	1131.956909	16.539955
28.800508	1121.886363	16.544973
28.662603	1120.851010	16.549991
28.942353	1128.239487	16.555008
28.665490	1130.271911	16.560026
28.624469	1130.959033	16.565043
28.976879	1123.867518	16.570061
28.782199	1122.805740	16.575079
28.915128	1129.875629	16.580096
29.049173	1110.714829	16.585114
28.676015	1105.988260	16.590131
28.547150	1098.586700	16.595149
28.645652	1118.617291	16.600167
29.009980	1119.921519	16.605184
28.691254	1122.915168	16.610202
28.845443	1129.963033	16.615219
29.098829	1117.379463	16.620237
28.757483	1125.644375	16.625255
28.861157	1123.179309	16.630272
29.172317	1114.528152	16.635290
29.225963	1122.847339	16.640307
29.304174	1115.937052	16.645325
28.974255	1115.174036	16.650343
29.300194	1119.825438	16.655360
29.834997	1112.701758	16.660378
29.219661	1129.114093	16.665395
29.027152	1117.749983	16.670413
28.894737	1115.727539	16.675431
29.275221	1115.818113	16.680448
29.170408	1110.219976	16.685466
29.300564	1126.591147	16.690483
29.453432	1128.946494	16.695501
29.658222	1138.365816	16.700519
29.928846	1140.778829	16.705536
29.694336	1113.695488	16.710554
29.318353	1113.566060	16.715571
29.301522	1118.714753	16.720589
29.723635	1129.034663	16.725607
29.920570	1143.344871	16.730624
29.876367	1133.873838	16.735642
29.845613	1120.599153	16.740659
29.980780	1112.805061	16.745677
29.760350	1104.862775	16.750695
29.796476	1101.164851	16.755712
30.034994	1092.945010	16.760730
29.645176	1095.928379	16.765747
29.732279	1088.295008	16.770765
29.805943	1107.716337	16.775783
29.937114	1122.549206	16.780800
29.958603	1128.917102	16.785818
29.643816	1147.293394	16.790835
29.954112	1132.305594	16.795853
30.377864	1131.858709	16.800871
30.238956	1135.529252	16.805888
30.637521	1123.207848	16.810906
30.362047	1133.649176	16.815923
30.150881	1119.318973	16.820941
30.118903	1110.447482	16.825959
30.021614	1128.504285	16.830976
30.350822	1132.987833	16.835994
29.873995	1135.220291	16.841011
30.186269	1130.302662	16.846029
30.542875	1135.981629	16.851047
30.171614	1132.517684	16.856064
30.303181	1128.587029	16.861082
30.206627	1134.057184	16.866099
30.251820	1137.655513	16.871117
30.299629	1132.828523	16.876135
30.368248	1124.834822	16.881152
30.470531	1125.435619	16.886170
30.075303	1132.152428	16.891187
30.373777	1136.032821	16.896205
30.485435	1157.485641	16.901223
30.558398	1150.880134	16.906240
30.948926	1147.869158	16.911258
30.430821	1151.768236	16.916275
30.598019	1147.074223	16.921293
30.602983	1146.928171	16.926311
30.674962	1155.517164	16.931328
31.118491	1148.693217	16.936346
30.975764	1154.323382	16.941363
30.970214	1150.666597	16.946381
30.958448	1148.778496	16.951399
30.817539	1151.019111	16.956416
31.073116	1149.463106	16.961434
30.913654	1152.723292	16.966451
31.050683	1150.396394	16.971469
31.140877	1150.827546	16.976487
31.054903	1150.146965	16.981504
31.302871	1135.898589	16.986522
31.089582	1153.148281	16.991539
31.195074	1145.062246	16.996557
31.018560	1150.891698	17.001575
30.726306	1142.455792	17.006592
31.489685	1146.283221	17.011610
31.002629	1147.117820	17.016627
31.289025	1169.620424	17.021645
31.429335	1167.421322	17.026663
31.169693	1180.324541	17.031680
31.133640	1165.835382	17.036698
31.338016	1173.653669	17.041715
31.548266	1173.846840	17.046733
31.886551	1173.505836	17.051751
31.490708	1178.281889	17.056768
31.580270	1171.385446	17.061786
31.483450	1176.620235	17.066803
31.902822	1176.122895	17.071821
31.817363	1174.979251	17.076839
31.350579	1174.737696	17.081856
31.776538	1169.358333	17.086874
31.587242	1172.563229	17.091891
31.596726	1176.404873	17.096909
31.906254	1165.772530	17.101927
31.827898	1169.802727	17.106944
31.926115	1166.047658	17.111962
32.006226	1175.064828	17.116979
31.402684	1173.276287	17.121997
31.745748	1175.892263	17.127015
31.781571	1200.699318	17.132032
32.087795	1191.887131	17.137050
32.065882	1203.778596	17.142067
32.440980	1199.292261	17.147085
32.569133	1190.656405	17.152103
32.118297	1191.107068	17.157120
32.575850	1188.855433	17.162138
32.383142	1197.228837	17.167155
32.528879	1200.195198	17.172173
32.401615	1198.650220	17.177191
32.534942	1192.691371	17.182208
32.807123	1184.785582	17.187226
32.292702	1175.446320	17.192243
32.433153	1166.023822	17.197261
32.413825	1159.658389	17.202279
32.109943	1166.923847	17.207296
32.362400	1170.415426	17.212314
32.883032	1181.909569	17.217331
32.861146	1193.123486	17.222349
32.821328	1185.294160	17.227367
32.732807	1190.702378	17.232384
33.100417	1182.584338	17.237402
32.634726	1170.481985	17.242419
32.193418	1163.826987	17.247437
32.951137	1179.746281	17.252455
32.452963	1189.771388	17.257472
32.926801	1179.100018	17.262490
32.957923	1194.138493	17.267507
32.958852	1185.764643	17.272525
33.003807	1186.219428	17.277543
32.914052	1189.353516	17.282560
33.282514	1187.912670	17.287578
32.847597	1195.474633	17.292595
32.956586	1184.959338	17.297613
33.290464	1183.969479	17.302631
33.164322	1184.229768	17.307648
33.109010	1186.808171	17.312666
33.348525	1189.196029	17.317683
33.048479	1190.010293	17.322701
33.032586	1180.988859	17.327719
32.973595	1187.548051	17.332736
32.893494	1185.616932	17.337754
32.945647	1184.408376	17.342771
33.003546	1190.427367	17.347789
33.292514	1197.564753	17.352807
32.926847	1217.488479	17.357824
33.154382	1221.773541	17.362842
33.512656	1219.515113	17.367859
33.203650	1224.024447	17.372877
33.726739	1210.762698	17.377895
33.486942	1216.540056	17.382912
33.789735	1209.106336	17.387930
33.718180	1213.029122	17.392947
33.632233	1217.724347	17.397965
33.658676	1208.619512	17.402983
33.765563	1209.894724	17.408000
33.741616	1219.769281	17.413018
33.954190	1214.534681	17.418035
33.510216	1210.318609	17.423053
34.009563	1222.196609	17.428071
34.025871	1233.864846	17.433088
34.161702	1236.545068	17.438106
33.949659	1232.459872	17.443123
33.834843	1234.680431	17.448141
34.165318	1226.737410	17.453159
34.356202	1238.749174	17.458176
34.113707	1234.589494	17.463194
34.547029	1240.056591	17.468211
34.110103	1225.160147	17.473229
34.390238	1232.616324	17.478247
34.150266	1234.195423	17.483264
34.262441	1234.472548	17.488282
34.451402	1231.550049	17.493299
34.397568	1234.757724	17.498317
34.544453	1236.624329	17.503335
34.647042	1233.577159	17.508352
34.662191	1231.703882	17.513370
34.438329	1229.908762	17.518387
34.206462	1235.461199	17.523405
34.740990	1236.107354	17.528423
34.533142	1230.764021	17.533440
34.551360	1227.428077	17.538458
34.692968	1232.510810	17.543475
34.662650	1233.870946	17.548493
34.540544	1221.958897	17.553511
34.510698	1233.760758	17.558528
34.731527	1222.710793	17.563546
35.026304	1227.106766	17.568563
34.672182	1230.807850	17.573581
35.060729	1223.163079	17.578599
34.912776	1230.653134	17.583616
34.773572	1227.754660	17.588634
34.953453	1230.304362	17.593651
34.781329	1236.169338	17.598669
34.944213	1222.720381	17.603687
34.830377	1236.523096	17.608704
34.980953	1252.558746	17.613722
35.345815	1257.218312	17.618739
35.263298	1250.340091	17.623757
35.470567	1251.870331	17.628775
35.633927	1251.085863	17.633792
35.362621	1238.625689	17.638810
35.153006	1223.210125	17.643827
35.329684	1233.800266	17.648845
35.610976	1245.562034	17.653863
35.484851	1241.969680	17.658880
35.524421	1241.022251	17.663898
35.496830	1241.120164	17.668915
35.678248	1244.528643	17.673933
35.644264	1240.607262	17.678951
35.728035	1255.555586	17.683968
35.495053	1250.046728	17.688986
35.708527	1251.100365	17.694003
35.712585	1245.952247	17.699021
35.846010	1249.092305	17.704039
35.892904	1253.940736	17.709056
35.844910	1250.529925	17.714074
35.835588	1245.575357	17.719091
35.675163	1236.902222	17.724109
36.065750	1243.381878	17.729127
35.982434	1245.681078	17.734144
36.080220	1247.681795	17.739162
36.166403	1250.369453	17.744179
35.925295	1248.566557	17.749197
36.056781	1243.170576	17.754215
35.922227	1246.931366	17.759232
36.148098	1254.061117	17.764250
36.059964	1240.076166	17.769267
36.230484	1240.557011	17.774285
36.212292	1242.348985	17.779303
36.376358	1241.770694	17.784320
36.159726	1252.603134	17.789338
36.497473	1248.628466	17.794355
35.931739	1250.087496	17.799373
36.271065	1249.137675	17.804391
36.420469	1265.994768	17.809408
36.399127	1273.516240	17.814426
36.551051	1273.169479	17.819443
36.766929	1276.638400	17.824461
36.980821	1272.598410	17.829479
36.939317	1267.321613	17.834496
36.664636	1272.720921	17.839514
36.635408	1274.023008	17.844531
36.591206	1276.978710	17.849549
36.633367	1268.280674	17.854567
36.541346	1268.471143	17.859584
36.555067	1275.455722	17.864602
36.840452	1264.445431	17.869619
36.523564	1272.281579	17.874637
37.029996	1283.955310	17.879655
37.159733	1295.872128	17.884672
36.974472	1308.890693	17.889690
37.670274	1291.486211	17.894707
37.123785	1283.541525	17.899725
37.265608	1270.452696	17.904743
37.247122	1268.864897	17.909760
37.141364	1270.108792	17.914778
37.190242	1264.619792	17.919795
37.283018	1290.466350	17.924813
37.295784	1291.248900	17.929831
37.198365	1292.923688	17.934848
37.317191	1293.006018	17.939866
37.669848	1293.217735	17.944883
37.525697	1292.392847	17.949901
37.720715	1290.815361	17.954919
37.785745	1292.727023	17.959936
37.903249	1291.944634	17.964954
37.777961	1289.313129	17.969971
37.771358	1284.381718	17.974989
37.766192	1290.978891	17.980007
37.862622	1287.386683	17.985024
37.674022	1285.701462	17.990042
38.146961	1287.570777	17.995059
38.031627	1271.768303	18.000077
37.539791	1260.056024	18.005095
37.795272	1275.553871	18.010112
37.821325	1279.470354	18.015130
38.024053	1281.509997	18.020147
37.923567	1287.832802	18.025165
38.269859	1275.697094	18.030183
38.035578	1282.350704	18.035200
37.779861	1277.179450	18.040218
38.088399	1281.132622	18.045235
38.334983	1282.700055	18.050253
38.049293	1283.102508	18.055271
38.130645	1286.420089	18.060288
37.829553	1285.298756	18.065306
38.234542	1290.043811	18.070323
38.118984	1303.903563	18.075341
38.197016	1308.107502	18.080359
38.510950	1311.214927	18.085376
38.663025	1314.786545	18.090394
38.271328	1304.969019	18.095411
38.314072	1312.600761	18.100429
38.256694	1313.526420	18.105447
38.604912	1308.353971	18.110464
38.288656	1312.359820	18.115482
38.827140	1329.978522	18.120499
39.015767	1335.539319	18.125517
38.905639	1333.201745	18.130535
39.282680	1337.268782	18.135552
38.726980	1330.522024	18.140570
39.073727	1328.536743	18.145587
39.173506	1326.244333	18.150605
39.543648	1321.004865	18.155623
38.990959	1307.463696	18.160640
38.811991	1301.383292	18.165658
39.036880	1304.908206	18.170675
39.404392	1322.776464	18.175693
39.359739	1331.831707	18.180711
39.375923	1329.985017	18.185728
39.385693	1329.888166	18.190746
39.458118	1322.189789	18.195763
39.408061	1332.420307	18.200781
39.358658	1329.230967	18.205799
39.122268	1324.415150	18.210816
38.999653	1331.756179	18.215834
39.396011	1322.491209	18.220851
39.593133	1324.422733	18.225869
39.728185	1321.278047	18.230887
39.637235	1318.249522	18.235904
39.465895	1325.788769	18.240922
39.748255	1318.412316	18.245939
39.380379	1319.351988	18.250957
39.367265	1330.024408	18.255975
39.554447	1335.224429	18.260992
39.624296	1347.683474	18.266010
40.280238	1353.081468	18.271027
40.169118	1350.014939	18.276045
40.141870	1353.097372	18.281063
40.374876	1344.326749	18.286080
40.170373	1342.829191	18.291098
40.040680	1326.469603	18.296115
40.185729	1332.082102	18.301133
40.112910	1333.136694	18.306151
40.337048	1342.583252	18.311168
40.564951	1348.874148	18.316186
40.172208	1323.744153	18.321203
40.224586	1336.858823	18.326221
40.402328	1335.964885	18.331239
40.535863	1337.986072	18.336256
40.488961	1346.943667	18.341274
40.439126	1340.264714	18.346291
40.408709	1344.005135	18.351309
40.357663	1343.942369	18.356327
40.775861	1328.363692	18.361344
40.828390	1339.974833	18.366362
40.724770	1335.744494	18.371379
40.869310	1330.017195	18.376397
40.470570	1335.644935	18.381415
40.941256	1335.520188	18.386432
40.892318	1335.131884	18.391450
40.764514	1337.900658	18.396467
40.683018	1336.165809	18.401485
40.667323	1336.086166	18.406503
40.732283	1334.599894	18.411520
40.757285	1337.878392	18.416538
40.769697	1339.196424	18.421555
41.276544	1352.492148	18.426573
41.086893	1364.824888	18.431591
41.418199	1360.106394	18.436608
41.206939	1371.713207	18.441626
41.446038	1363.593912	18.446643
41.203511	1370.622145	18.451661
41.169794	1365.338514	18.456679
41.404467	1364.561523	18.461696
41.559444	1365.333128	18.466714
41.519033	1366.047718	18.471731
41.356975	1364.939183	18.476749
41.474047	1368.321338	18.481767
41.656477	1367.019545	18.486784
41.387187	1373.482538	18.491802
41.602353	1365.289254	18.496819
41.638934	1366.323372	18.501837
41.327035	1363.400319	18.506855
41.924090	1378.667305	18.511872
41.842644	1390.878608	18.516890
42.118609	1393.197866	18.521907
41.941534	1393.487457	18.526925
42.002102	1383.356022	18.531943
42.336538	1384.097913	18.536960
41.922056	1383.291799	18.541978
42.104835	1387.836281	18.546995
42.347977	1379.967485	18.552013
42.272479	1386.354695	18.557031
42.529124	1383.206399	18.562048
42.343279	1385.626137	18.567066
42.607908	1378.668725	18.572083
42.440331	1384.007818	18.577101
42.424728	1391.438241	18.582119
42.614461	1380.985820	18.587136
42.545276	1379.719784	18.592154
42.684157	1379.700764	18.597171
42.421225	1372.701971	18.602189
42.180459	1376.742185	18.607207
42.410914	1376.939888	18.612224
42.533714	1380.568336	18.617242
42.714463	1383.090755	18.622259
43.019735	1382.761119	18.627277
42.591412	1391.768511	18.632295
42.779985	1391.042459	18.637312
42.553261	1385.916760	18.642330
42.717528	1382.494789	18.647347
42.679819	1382.939647	18.652365
42.323945	1389.590602	18.657383
42.939028	1396.352042	18.662400
42.921419	1408.733493	18.667418
42.988962	1419.591041	18.672435
43.236513	1404.405104	18.677453
43.323670	1415.185781	18.682471
43.052947	1413.615717	18.687488
43.093561	1416.507796	18.692506
42.933132	1406.236171	18.697523
43.363815	1408.723904	18.702541
43.234045	1410.963892	18.707559
43.054566	1413.936508	18.712576
43.519457	1431.527749	18.717594
43.666315	1439.186408	18.722611
43.909271	1431.921149	18.727629
43.668725	1439.129396	18.732647
44.210545	1432.598102	18.737664
44.045426	1433.573890	18.742682
43.427701	1420.378817	18.747699
43.909501	1414.902330	18.752717
43.946682	1421.722464	18.757735
44.086285	1426.985905	18.762752
43.764176	1431.556128	18.767770
43.892710	1431.279772	18.772787
44.307300	1424.050663	18.777805
43.967475	1425.820719	18.782823
44.068397	1433.912958	18.787840
44.131011	1428.652330	18.792858
43.883850	1428.672429	18.797875
44.083309	1421.652955	18.802893
43.944763	1424.440058	18.807911
44.081237	1425.200163	18.812928
44.119191	1427.979694	18.817946
44.423632	1448.037636	18.822963
44.600533	1453.206723	18.827981
44.364073	1463.785117	18.832999
44.507325	1446.627858	18.838016
44.581057	1450.338855	18.843034
44.799091	1453.105502	18.848051
45.136432	1448.498579	18.853069
44.791559	1453.770204	18.858087
45.143349	1450.218744	18.863104
44.908990	1448.688324	18.868122
45.004726	1447.109152	18.873139
44.996410	1443.498425	18.878157
45.108468	1444.282653	18.883175
45.106715	1445.708549	18.888192
45.009112	1448.292029	18.893210
45.018570	1446.437385	18.898227
45.368598	1444.918861	18.903245
45.076067	1447.699576	18.908263
44.827068	1441.259065	18.913280
44.946615	1452.051333	18.918298
45.124212	1447.559048	18.923315
45.205358	1441.631579	18.928333
45.200561	1453.406625	18.933351
45.698093	1441.950064	18.938368
45.349516	1445.503431	18.943386
45.082759	1444.293331	18.948403
45.237629	1438.857584	18.953421
45.149408	1456.549888	18.958439
45.527194	1460.785336	18.963456
45.403405	1474.358812	18.968474
45.559169	1475.217693	18.973491
45.535591	1461.902551	18.978509
45.604570	1472.496910	18.983527
45.361924	1464.078203	18.988544
45.354740	1475.326897	18.993562
45.633032	1493.890825	18.998579
46.079483	1490.348486	19.003597
45.924402	1495.235554	19.008615
46.096241	1496.602397	19.013632
46.374850	1494.926799	19.018650
46.282115	1492.684745	19.023667
46.201567	1486.957257	19.028685
46.263323	1486.184878	19.033703
46.126816	1484.922893	19.038720
46.404392	1489.274940	19.043738
46.093331	1490.167813	19.048755
46.417112	1485.073367	19.053773
46.425466	1489.671958	19.058791
46.776953	1500.927817	19.063808
46.846757	1507.723689	19.068826
46.622577	1502.877842	19.073843
47.045329	1496.042225	19.078861
46.539569	1496.461831	19.083879
46.800643	1505.099235	19.088896
47.000947	1502.223232	19.093914
46.889371	1516.097475	19.098931
47.192724	1500.519926	19.103949
46.863206	1508.657886	19.108967
47.231300	1509.415076	19.113984
47.358727	1514.962056	19.119002
47.407746	1504.802534	19.124019
47.174824	1481.009188	19.129037
46.898964	1491.357513	19.134055
47.143658	1492.941030	19.139072
47.397019	1502.748197	19.144090
47.386507	1511.707736	19.149107
47.621648	1501.310707	19.154125
47.534937	1513.207628	19.159143
47.429750	1511.982975	19.164160
47.356468	1507.358200	19.169178
47.371473	1505.704595	19.174195
47.505915	1506.361105	19.179213
47.093385	1513.097083	19.184231
47.170666	1499.320332	19.189248
47.763194	1502.991896	19.194266
47.575755	1520.886920	19.199283
47.567580	1527.262647	19.204301
47.771235	1539.391821	19.209319
48.222996	1533.230117	19.214336
48.217769	1532.269616	19.219354
47.778791	1543.695761	19.224371
48.062511	1534.598133	19.229389
48.093972	1533.192979	19.234407
48.286926	1537.949993	19.239424
48.612989	1528.446149	19.244442
48.341294	1530.567137	19.249459
48.424254	1529.542821	19.254477
48.236150	1522.945345	19.259495
48.255197	1528.236657	19.264512
48.699883	1534.390160	19.269530
48.268070	1536.870728	19.274547
48.603392	1520.987868	19.279565
48.806524	1533.273815	19.284583
48.764287	1525.915972	19.289600
48.607218	1525.525489	19.294618
48.589858	1522.868198	19.299635
48.782491	1517.911598	19.304653
48.675079	1525.156108	19.309671
48.619204	1516.469048	19.314688
49.195679	1531.720303	19.319706
48.783995	1532.067640	19.324723
48.721112	1531.767072	19.329741
48.939595	1540.237928	19.334759
48.828175	1540.167835	19.339776
49.264722	1547.498663	19.344794
49.162868	1537.077883	19.349811
49.257553	1534.545344	19.354829
49.232610	1542.102187	19.359847
49.253956	1539.127464	19.364864
49.488255	1540.847351	19.369882
49.453363	1543.078735	19.374899
49.631635	1539.484728	19.379917
49.635651	1543.643901	19.384935
49.689586	1540.699608	19.389952
49.668194	1547.337372	19.394970
49.399678	1545.595671	19.399987
49.510896	1543.193856	19.405005
49.609739	1549.979033	19.410023
49.492181	1571.320383	19.415040
49.912469	1565.039864	19.420058
49.936893	1572.384219	19.425075
49.930965	1570.892340	19.430093
49.911907	1570.169951	19.435111
49.911073	1566.059536	19.440128
50.111937	1567.440871	19.445146
49.991705	1574.026115	19.450163
49.903205	1572.696726	19.455181
50.193235	1566.155887	19.460199
50.296109	1587.872962	19.465216
51.039283	1587.068062	19.470234
50.726699	1583.562801	19.475251
50.719502	1569.331082	19.480269
50.832018	1562.731843	19.485287
50.363160	1568.740564	19.490304
50.677803	1560.927947	19.495322
50.578526	1564.449510	19.500339
50.783621	1575.678089	19.505357
50.835831	1581.403688	19.510375
50.920117	1598.770742	19.515392
50.937916	1587.784845	19.520410
50.878054	1598.206531	19.525427
50.832693	1590.798387	19.530445
50.683658	1590.982945	19.535463
51.051737	1590.181099	19.540480
51.402053	1582.507839	19.545498
50.887809	1584.605609	19.550515
50.989993	1582.185993	19.555533
51.653979	1576.100549	19.560551
51.452167	1587.399662	19.565568
51.553861	1577.754988	19.570586
51.411493	1587.916314	19.575603
51.379979	1578.653930	19.580621
51.698646	1583.872422	19.585639
51.388809	1590.863474	19.590656
51.561115	1581.967730	19.595674
51.304325	1603.573515	19.600691
51.514343	1610.211965	19.605709
51.774247	1613.304384	19.610727
51.641350	1610.709516	19.615744
51.495729	1608.268722	19.620762
51.192653	1618.085814	19.625779
51.520032	1632.415429	19.630797
52.059815	1633.789470	19.635815
52.005795	1643.008650	19.640832
52.042750	1643.797843	19.645850
52.112370	1648.326494	19.650867
52.130931	1637.779017	19.655885
52.293218	1647.888757	19.660903
52.071425	1652.166843	19.665920
52.452190	1640.755456	19.670938
52.693715	1632.171449	19.675955
52.608660	1631.036759	19.680973
52.407514	1629.211846	19.685991
52.448556	1634.327899	19.691008
52.770271	1627.918796	19.696026
52.830152	1623.615242	19.701043
52.790025	1636.964379	19.706061
53.026753	1626.405588	19.711079
52.546636	1630.339436	19.716096
53.063816	1634.089256	19.721114
53.018637	1651.268358	19.726131
53.084110	1646.143010	19.731149
53.104051	1646.573998	19.736167
53.027900	1665.736189	19.741184
53.291455	1658.837886	19.746202
53.340771	1659.704560	19.751219
53.604756	1659.805377	19.756237
53.460970	1656.175299	19.761255
53.372482	1653.867558	19.766272
53.948553	1639.156128	19.771290
53.547206	1638.168296	19.776307
53.508331	1638.464142	19.781325
53.909024	1638.619881	19.786343
53.636213	1649.750087	19.791360
54.003557	1641.464926	19.796378
53.799187	1635.278360	19.801395
53.481966	1641.659637	19.806413
53.962994	1647.595752	19.811431
53.947119	1647.468893	19.816448
53.905902	1651.630860	19.821466
53.767711	1644.943177	19.826483
53.855022	1655.817303	19.831501
54.174821	1646.577810	19.836519
53.918500	1647.704538	19.841536
53.829572	1648.931109	19.846554
54.005471	1662.006704	19.851571
54.331193	1664.512646	19.856589
54.430587	1662.499384	19.861607
54.231705	1675.089803	19.866624
54.204358	1671.307372	19.871642
54.493152	1670.475737	19.876659
54.786467	1663.433527	19.881677
54.362603	1663.728159	19.886695
54.038027	1671.689008	19.891712
54.213367	1677.643467	19.896730
54.884201	1691.163512	19.901747
54.918071	1688.978813	19.906765
55.213570	1691.059843	19.911783
55.097880	1700.959346	19.916800
55.498705	1693.588692	19.921818
55.713411	1692.177198	19.926835
55.408480	1705.431264	19.931853
55.198061	1679.718925	19.936871
55.247588	1691.742637	19.941888
55.277580	1686.507795	19.946906
55.405844	1693.028322	19.951923
55.417948	1689.078724	19.956941
55.672910	1687.553479	19.961959
55.351574	1698.251597	19.966976
55.456634	1696.260620	19.971994
55.428263	1690.840953	19.977011
55.487737	1687.475243	19.982029
55.767931	1681.508819	19.987047
55.396491	1683.969570	19.992064
55.836927	1682.566764	19.997082
55.687274	1679.535682	20.002099
55.834054	1687.327942	20.007117
55.957390	1690.478029	20.012135
56.113444	1700.475450	20.017152
55.871639	1715.622614	20.022170
56.027008	1706.896139	20.027187
56.224416	1717.031212	20.032205
56.312806	1701.090630	20.037223
56.235874	1705.815218	20.042240
56.424055	1709.530949	20.047258
56.784143	1712.887115	20.052275
56.422585	1707.385209	20.057293
56.661566	1693.100803	20.062311
56.504999	1708.833060	20.067328
56.603087	1701.787332	20.072346
56.710641	1698.569171	20.077363
56.524959	1706.137748	20.082381
56.733601	1704.352454	20.087399
56.691377	1723.427997	20.092416
56.849310	1723.567241	20.097434
57.342085	1734.989641	20.102451
57.149812	1737.242781	20.107469
57.046504	1731.249286	20.112487
56.953325	1732.220267	20.117504
57.465003	1729.983613	20.122522
57.350538	1733.562060	20.127539
57.354402	1739.545723	20.132557
57.697945	1727.172323	20.137575
57.427337	1725.073860	20.142592
57.389016	1718.792050	20.147610
57.590139	1724.576117	20.152627
57.648074	1721.629553	20.157645
57.703910	1716.764438	20.162663
57.300597	1728.304497	20.167680
57.532913	1729.220402	20.172698
57.832770	1732.993633	20.177715
58.107305	1753.777398	20.182733
58.222661	1747.345721	20.187751
58.184969	1750.946893	20.192768
57.990635	1755.684636	20.197786
58.222948	1757.563145	20.202803
58.108542	1757.545120	20.207821
58.163729	1753.662388	20.212839
58.195355	1754.241838	20.217856
58.113024	1752.800388	20.222874
58.275723	1749.227021	20.227891
58.400315	1763.226948	20.232909
58.164618	1751.264794	20.237927
58.090545	1766.638174	20.242944
58.332998	1769.410678	20.247962
58.692689	1775.924810	20.252979
58.673565	1776.893769	20.257997
59.177470	1768.910340	20.263015
59.384689	1782.993848	20.268032
59.200968	1781.529812	20.273050
59.353463	1769.192343	20.278067
58.962411	1773.943766	20.283085
59.293074	1768.021709	20.288103
59.256655	1768.738018	20.293120
59.516039	1767.535656	20.298138
59.551576	1769.519189	20.303155
59.372783	1780.033131	20.308173
59.522692	1763.007491	20.313191
59.441599	1766.066639	20.318208
59.617135	1766.952184	20.323226
59.223999	1768.165354	20.328243
59.050571	1768.638206	20.333261
59.611004	1768.406080	20.338279
59.592363	1767.687156	20.343296
59.682012	1776.937351	20.348314
59.811961	1784.735990	20.353331
59.896634	1781.760972	20.358349
60.064375	1783.620255	20.363367
59.830328	1787.003946	20.368384
59.771762	1793.863326	20.373402
60.096234	1790.948207	20.378419
59.942024	1798.321460	20.383437
60.231701	1786.606149	20.388455
60.113727	1793.266309	20.393472
60.138698	1812.215480	20.398490
60.426120	1804.872606	20.403507
60.272758	1816.061893	20.408525
60.578560	1812.747103	20.413543
60.578326	1816.972014	20.418560
60.419512	1815.382590	20.423578
60.732301	1810.088284	20.428595
60.616817	1821.582328	20.433613
61.048793	1805.604434	20.438631
60.797460	1814.139452	20.443648
60.524146	1826.971848	20.448666
61.047375	1830.838433	20.453683
60.841063	1837.462451	20.458701
61.055380	1829.318671	20.463719
61.478217	1834.520001	20.468736
61.645522	1835.448646	20.473754
61.762660	1836.521426	20.478771
61.210630	1841.313302	20.483789
61.557388	1834.918866	20.488807
61.498362	1834.503872	20.493824
61.579483	1835.000720	20.498842
61.973883	1814.757351	20.503859
61.744965	1837.460822	20.508877
61.633334	1831.641108	20.513895
61.914438	1830.367429	20.518912
61.656027	1829.541744	20.523930
61.885411	1842.560998	20.528947
62.043021	1855.946481	20.533965
62.159832	1850.501932	20.538983
62.346078	1855.247557	20.544000
61.987831	1858.416392	20.549018
62.421932	1854.206327	20.554035
62.326142	1859.129361	20.559053
62.483478	1853.486760	20.564071
62.630342	1846.816358	20.569088
62.537285	1853.018477	20.574106
62.347424	1840.770315	20.579123
62.204598	1853.843728	20.584141
63.024279	1853.232452	20.589159
62.782296	1847.595341	20.594176
62.723893	1857.394119	20.599194
63.080954	1859.938213	20.604211
62.860719	1874.903219	20.609229
62.547230	1875.603203	20.614247
63.028854	1870.157298	20.619264
63.457099	1873.866786	20.624282
63.405852	1874.417049	20.629299
63.355634	1866.074528	20.634317
63.479398	1860.296931	20.639335
63.522696	1861.043746	20.644352
63.461622	1862.775569	20.649370
63.720526	1863.585111	20.654387
63.870700	1860.826006	20.659405
63.899382	1869.373353	20.664423
63.929563	1854.291079	20.669440
63.567684	1854.988839	20.674458
64.033817	1854.530199	20.679475
64.090798	1856.220426	20.684493
64.046443	1850.790357	20.689511
64.236017	1858.145692	20.694528
64.203919	1856.458117	20.699546
64.353313	1851.376286	20.704563
64.419055	1852.862698	20.709581
64.555731	1850.792451	20.714599
64.383703	1858.062776	20.719616
64.325874	1858.383811	20.724634
64.365869	1848.195636	20.729651
64.312084	1849.083330	20.734669
64.258221	1843.394599	20.739687
64.463230	1842.666593	20.744704
64.001805	1855.206534	20.749722
64.387136	1866.881471	20.754739
64.526203	1876.171182	20.759757
64.445011	1885.750126	20.764775
64.633255	1880.777209	20.769792
64.806828	1902.496405	20.774810
64.980101	1906.820173	20.779827
64.822562	1906.479363	20.784845
65.170559	1901.406759	20.789863
65.545062	1906.221230	20.794880
65.006043	1904.988848	20.799898
65.110606	1905.353075	20.804915
65.477620	1902.707274	20.809933
65.746577	1924.630002	20.814951
65.938808	1919.357196	20.819968
65.415875	1919.570594	20.824986
65.949722	1918.529079	20.830003
65.787877	1928.219830	20.835021
65.717586	1928.932700	20.840039
66.133698	1920.753491	20.845056
66.336968	1928.718805	20.850074
66.136368	1925.722489	20.855091
66.207029	1929.319935	20.860109
66.218562	1921.135667	20.865127
66.478762	1922.857215	20.870144
66.450877	1923.710703	20.875162
66.620965	1933.179566	20.880179
66.764854	1921.778454	20.885197
66.505290	1925.238448	20.890215
66.482817	1924.267786	20.895232
66.454068	1927.068294	20.900250
66.446144	1928.281081	20.905267
66.344962	1923.519066	20.910285
66.697443	1946.083910	20.915303
66.902332	1946.497276	20.920320
66.597886	1947.829634	20.925338
66.698041	1944.355163	20.930355
67.076151	1943.072500	20.935373
66.772932	1953.702831	20.940391
67.083916	1947.654829	20.945408
66.968195	1972.570891	20.950426
67.546566	1973.252346	20.955443
67.493756	1975.530853	20.960461
67.346442	1975.952929	20.965479
67.877366	1969.787398	20.970496
67.564815	1976.064886	20.975514
67.747858	1969.415213	20.980531
67.774605	1965.274928	20.985549
67.799277	1964.278347	20.990567
68.061253	1968.094917	20.995584
67.893295	1978.755626	21.000602
68.114886	1959.284789	21.005619
68.051017	1962.697822	21.010637
68.001768	1965.955676	21.015655
68.133950	1983.769964	21.020672
68.173220	1993.490056	21.025690
68.390501	1993.300573	21.030707
68.567112	1986.514161	21.035725
68.773534	1981.102761	21.040743
69.119288	1978.484090	21.045760
68.801497	1978.989906	21.050778
68.593838	1984.771281	21.055795
68.837254	1975.588730	21.060813
68.856268	1988.583490	21.065831
68.789201	1973.253419	21.070848
68.864742	1981.571804	21.075866
68.872341	1978.710299	21.080883
69.201740	1972.500180	21.085901
69.273618	1976.805716	21.090919
69.317602	1976.515004	21.095936
69.107456	1974.268697	21.100954
69.169737	1975.263953	21.105971
69.169520	1994.445475	21.110989
69.292149	2009.840070	21.116007
69.258996	2008.791641	21.121024
69.436006	2005.229234	21.126042
69.121765	2000.035928	21.131059
70.019916	2015.107236	21.136077
69.836245	2026.302086	21.141095
70.003641	2031.568613	21.146112
70.063823	2025.542816	21.151130
69.910715	2026.770987	21.156147
70.251773	2026.488173	21.161165
69.847177	2031.002147	21.166183
70.466731	2024.130960	21.171200
70.399444	2037.184145	21.176218
70.101490	2031.539698	21.181235
70.205478	2035.969070	21.186253
70.498424	2045.146787	21.191271
70.755787	2046.713698	21.196288
70.531346	2043.171294	21.201306
70.917716	2061.903448	21.206323
70.898961	2055.297389	21.211341
70.625874	2059.791958	21.216359
71.080827	2052.393276	21.221376
70.956274	2060.722787	21.226394
70.874777	2048.764399	21.231411
70.897217	2054.656523	21.236429
71.121601	2081.328693	21.241447
71.558067	2068.469548	21.246464
71.408160	2073.134281	21.251482
71.048313	2070.728883	21.256499
71.922635	2066.133266	21.261517
71.799514	2074.205455	21.266535
72.191843	2062.553651	21.271552
71.842122	2071.262584	21.276570
72.007209	2071.423089	21.281587
71.950745	2063.613792	21.286605
72.039563	2072.220980	21.291623
72.090416	2062.798602	21.296640
71.833594	2056.992213	21.301658
72.104492	2062.281772	21.306675
72.501922	2070.955186	21.311693
72.196770	2094.063395	21.316711
72.135461	2093.277897	21.321728
72.627514	2104.268398	21.326746
72.950140	2087.929966	21.331763
72.738367	2089.417074	21.336781
72.688824	2093.436833	21.341799
72.902151	2084.584012	21.346816
73.079802	2093.124926	21.351834
73.196175	2086.123242	21.356851
73.356891	2086.214391	21.361869
73.097733	2095.100866	21.366887
73.468866	2083.689964	21.371904
73.218793	2086.142885	21.376922
73.621311	2086.792831	21.381939
73.486697	2082.628050	21.386957
73.387745	2092.652199	21.391975
73.714782	2078.239866	21.396992
73.210031	2087.847726	21.402010
73.077847	2083.190010	21.407027
73.547517	2080.918137	21.412045
73.635710	2084.098140	21.417063
73.643917	2083.502712	21.422080
73.786326	2086.146560	21.427098
73.799407	2101.438909	21.432115
73.884830	2104.671738	21.437133
73.892693	2100.134928	21.442151
73.906837	2097.558151	21.447168
73.903113	2106.433049	21.452186
73.946625	2110.365356	21.457203
74.352814	2122.032703	21.462221
74.308502	2134.065602	21.467239
74.516104	2131.020950	21.472256
74.507393	2135.656023	21.477274
74.639841	2129.804052	21.482291
74.933854	2125.262376	21.487309
74.465858	2131.775511	21.492327
74.634859	2143.861291	21.497344
75.096284	2158.234556	21.502362
75.143993	2157.082569	21.507379
75.308494	2148.572057	21.512397
74.987054	2153.632943	21.517415
75.268828	2145.959339	21.522432
75.436187	2143.319784	21.527450
75.539011	2150.154961	21.532467
75.356185	2149.221071	21.537485
75.415222	2162.466837	21.542503
75.374745	2169.964745	21.547520
75.644497	2179.550726	21.552538
75.685469	2174.898959	21.557555
76.194026	2168.232709	21.562573
76.111106	2177.234936	21.567591
76.084302	2173.580249	21.572608
76.630799	2177.332832	21.577626
76.581200	2172.191717	21.582643
76.427059	2172.744853	21.587661
76.536857	2176.664627	21.592679
76.397308	2180.611513	21.597696
76.498329	2183.166953	21.602714
76.207497	2180.103240	21.607731
76.696499	2177.883667	21.612749
76.688283	2192.927656	21.617767
76.678227	2196.412935	21.622784
77.043224	2201.961380	21.627802
76.771138	2206.199517	21.632819
76.912326	2216.117054	21.637837
76.854596	2204.804631	21.642855
77.079430	2205.621803	21.647872
77.323086	2202.469589	21.652890
77.056027	2215.029211	21.657907
77.450818	2222.299953	21.662925
77.538634	2222.865787	21.667943
77.463443	2222.388102	21.672960
78.086178	2214.565488	21.677978
78.315105	2212.372042	21.682995
78.446388	2197.130172	21.688013
78.407393	2191.861699	21.693031
78.447602	2182.948113	21.698048
78.471818	2164.791235	21.703066
78.481760	2168.582260	21.708083
78.585940	2167.307927	21.713101
78.629451	2170.605979	21.718119
78.617528	2168.632343	21.723136
78.948283	2163.903071	21.728154
78.554346	2173.274518	21.733171
78.857731	2161.877138	21.738189
78.792792	2165.311653	21.743207
78.442177	2163.878756	21.748224
78.924951	2166.641072	21.753242
78.515441	2165.815975	21.758259
78.820678	2153.524961	21.763277
78.597770	2169.640332	21.768295
78.765955	2175.318996	21.773312
78.867070	2184.108074	21.778330
78.749778	2190.035984	21.783347
79.071057	2190.419457	21.788365
78.838081	2206.168804	21.793383
78.896601	2228.807931	21.798400
79.526559	2220.887658	21.803418
79.382849	2224.440349	21.808435
79.482778	2220.681593	21.813453
79.495456	2232.760647	21.818471
79.584338	2245.739723	21.823488
79.770698	2255.442318	21.828506
79.789460	2256.390466	21.833523
80.581692	2252.226908	21.838541
80.162273	2250.150648	21.843559
80.104419	2249.863799	21.848576
80.849916	2251.797958	21.853594
80.682922	2263.210696	21.858611
80.544288	2246.319708	21.863629
80.665330	2267.638257	21.868647
80.691981	2265.240491	21.873664
81.165068	2262.606597	21.878682
81.024318	2268.685277	21.883699
80.710132	2264.652938	21.888717
81.233699	2258.538909	21.893735
81.036275	2267.918034	21.898752
81.104551	2260.475007	21.903770
81.075081	2270.103107	21.908787
81.140612	2265.223616	21.913805
81.046481	2266.980249	21.918823
81.231070	2291.802217	21.923840
82.085909	2294.808476	21.928858
81.779572	2300.238968	21.933875
81.604831	2296.290230	21.938893
81.735951	2297.241038	21.943911
81.798659	2295.363301	21.948928
81.952667	2283.313768	21.953946
81.645698	2292.890974	21.958963
82.021266	2304.117843	21.963981
82.285987	2311.779469	21.968999
82.322589	2311.201379	21.974016
82.195234	2312.287507	21.979034
82.316413	2324.155352	21.984051
82.511248	2311.139158	21.989069
82.595486	2317.448726	21.994087
82.488052	2329.157175	21.999104
82.835564	2335.713328	22.004122
83.246312	2337.638354	22.009139
83.137525	2331.629784	22.014157
83.325769	2338.483974	22.019175
83.345883	2329.732298	22.024192
83.784865	2337.657616	22.029210
83.814943	2345.051009	22.034227
83.670012	2312.828872	22.039245
83.290874	2302.950356	22.044263
83.388925	2300.765575	22.049280
83.643029	2317.503327	22.054298
83.852643	2332.148378	22.059315
83.667666	2319.476176	22.064333
84.126556	2319.236845	22.069351
83.904582	2323.407265	22.074368
84.181052	2310.720087	22.079386
83.936493	2322.330365	22.084403
83.950477	2316.488882	22.089421
84.096263	2325.506874	22.094439
83.985273	2319.010859	22.099456
84.300345	2331.684829	22.104474
84.306760	2354.528050	22.109491
84.407393	2353.532647	22.114509
84.669545	2348.195361	22.119527
84.443402	2354.854772	22.124544
84.845414	2341.647550	22.129562
84.651558	2366.974048	22.134579
84.921281	2378.859075	22.139597
85.146836	2376.049602	22.144615
85.285838	2375.901819	22.149632
85.413622	2376.808300	22.154650
85.531623	2375.323385	22.159667
85.359095	2382.999565	22.164685
85.520997	2381.629433	22.169703
85.067693	2378.589825	22.174720
85.493806	2390.716695	22.179738
85.499369	2402.736820	22.184755
85.555926	2399.024574	22.189773
85.810761	2413.064157	22.194791
85.969592	2411.247660	22.199808
86.235708	2421.586790	22.204826
86.171944	2431.844712	22.209843
86.277005	2426.693260	22.214861
86.404714	2423.889349	22.219879
86.425953	2432.561865	22.224896
86.717576	2428.803999	22.229914
86.918998	2426.538302	22.234931
87.011570	2432.020514	22.239949
87.224288	2429.854920	22.244967
87.045683	2424.100799	22.249984
87.037946	2429.172827	22.255002
87.113096	2430.447098	22.260019
86.977973	2420.661182	22.265037
87.111730	2421.765899	22.270055
87.093163	2437.189809	22.275072
87.602867	2438.401974	22.280090
87.285855	2436.717806	22.285107
87.609832	2448.660836	22.290125
87.519567	2440.729381	22.295143
87.206016	2447.192269	22.300160
87.814735	2447.269878	22.305178
87.616029	2464.000079	22.310195
87.763404	2469.340547	22.315213
88.292922	2469.227322	22.320231
88.188320	2461.655727	22.325248
88.398984	2450.809342	22.330266
88.556172	2454.354394	22.335283
88.662355	2461.213563	22.340301
88.822113	2459.907956	22.345319
88.792563	2454.990209	22.350336
89.055237	2457.161432	22.355354
89.417733	2463.990370	22.360371
88.768122	2450.391398	22.365389
89.123578	2456.088767	22.370407
89.126511	2465.080490	22.375424
89.336717	2468.319902	22.380442
89.531534	2473.196588	22.385459
89.696773	2467.413474	22.390477
89.960700	2462.267992	22.395495
89.641212	2456.040704	22.400512
89.714994	2439.302139	22.405530
90.014841	2447.322601	22.410547
89.892511	2433.771781	22.415565
89.571562	2442.828928	22.420583
89.700108	2466.817502	22.425600
89.919760	2464.354284	22.430618
89.952695	2461.682599	22.435635
89.813572	2472.618412	22.440653
90.057411	2469.216890	22.445671
90.151034	2492.557711	22.450688
90.323352	2500.279613	22.455706
90.505759	2498.774180	22.460723
90.549884	2505.292838	22.465741
90.664842	2491.844026	22.470759
90.424995	2505.227371	22.475776
90.650677	2509.250883	22.480794
90.776991	2519.406522	22.485811
91.027421	2527.061566	22.490829
91.332816	2526.998048	22.495847
91.391788	2518.035098	22.500864
91.805504	2517.407555	22.505882
91.671221	2516.543955	22.510899
91.326203	2523.168392	22.515917
91.836159	2525.612478	22.520935
91.651874	2538.977596	22.525952
92.024850	2543.008228	22.530970
92.230578	2545.704668	22.535987
92.144443	2549.045526	22.541005
92.570873	2537.447177	22.546023
92.214907	2543.757670	22.551040
92.296745	2542.552757	22.556058
92.393451	2540.502030	22.561075
92.424789	2539.931890	22.566093
92.488308	2532.687169	22.571111
92.373617	2544.224531	22.576128
92.680928	2561.666374	22.581146
93.132072	2561.403913	22.586163
92.997304	2568.608946	22.591181
92.976569	2566.912325	22.596199
92.923808	2565.596617	22.601216
93.250656	2561.728945	22.606234
93.073695	2565.908119	22.611251
93.561307	2585.317097	22.616269
93.700465	2591.956286	22.621287
93.582927	2600.471548	22.626304
93.516113	2594.943356	22.631322
94.174001	2594.525003	22.636339
93.460403	2588.575918	22.641357
93.693113	2589.290621	22.646375
93.859568	2589.322553	22.651392
93.894442	2608.902589	22.656410
94.024955	2612.061126	22.661427
94.540471	2617.252892	22.666445
94.882717	2610.145067	22.671463
94.764938	2612.967526	22.676480
94.680356	2603.114857	22.681498
95.218403	2602.227341	22.686515
95.212855	2602.707855	22.691533
95.008327	2603.059099	22.696551
95.048738	2602.133497	22.701568
95.084146	2601.455982	22.706586
95.287613	2592.598206	22.711603
94.978877	2601.627830	22.716621
95.282803	2597.107214	22.721639
95.547596	2616.807076	22.726656
95.855133	2624.031428	22.731674
95.929536	2623.254930	22.736691
95.854542	2625.015915	22.741709
95.690708	2617.272545	22.746727
95.921837	2621.662923	22.751744
95.851642	2630.500304	22.756762
95.955169	2615.248447	22.761779
95.819249	2629.933272	22.766797
95.901212	2622.483868	22.771815
95.955880	2646.188083	22.776832
96.065848	2648.275554	22.781850
96.487859	2649.445167	22.786867
96.567719	2657.617129	22.791885
96.617776	2666.627152	22.796903
96.597248	2686.296778	22.801920
96.910578	2681.240295	22.806938
97.143919	2675.266684	22.811955
97.100950	2681.751014	22.816973
97.375022	2672.411789	22.821991
97.555699	2676.408149	22.827008
97.309495	2671.989226	22.832026
97.510310	2678.951335	22.837043
97.528186	2699.417032	22.842061
98.277586	2695.873485	22.847079
98.023636	2696.493167	22.852096
98.346047	2688.842100	22.857114
98.569268	2694.059845	22.862131
98.039609	2687.730637	22.867149
98.563146	2686.207685	22.872167
98.476452	2692.303565	22.877184
98.761727	2690.223960	22.882202
98.790858	2675.463919	22.887219
98.600369	2690.247212	22.892237
98.820153	2676.123757	22.897255
98.830697	2680.278610	22.902272
98.600016	2688.366168	22.907290
98.929530	2708.213708	22.912307
99.005308	2719.065291	22.917325
98.931068	2717.769663	22.922343
99.043483	2724.762178	22.927360
99.100189	2725.611940	22.932378
99.014126	2734.579181	22.937395
99.117187	2750.004918	22.942413
99.500889	2743.229169	22.947431
99.820592	2765.511246	22.952448
99.707729	2772.038290	22.957466
100.358861	2775.198070	22.962483
100.430136	2774.380742	22.967501
100.347091	2767.614540	22.972519
100.613294	2762.234315	22.977536
100.781774	2766.223269	22.982554
100.782266	2748.304299	22.987571
100.406812	2773.277246	22.992589
100.525426	2770.879138	22.997607
101.161201	2759.687332	23.002624
100.501342	2765.053279	23.007642
100.980480	2765.450793	23.012659
101.208233	2782.619424	23.017677
101.281332	2787.010422	23.022695
101.388793	2785.887475	23.027712
100.859502	2792.059430	23.032730
101.081040	2784.528568	23.037747
101.312523	2804.016844	23.042765
101.540522	2808.379052	23.047783
101.527496	2821.782597	23.052800
101.755421	2818.285597	23.057818
101.875843	2818.250737	23.062835
101.804124	2834.176789	23.067853
102.115852	2837.302219	23.072871
102.099930	2843.296670	23.077888
102.305003	2846.686629	23.082906
102.399633	2846.194195	23.087923
102.241182	2846.226375	23.092941
102.677747	2860.759147	23.097959
103.028280	2862.483960	23.102976
103.047545	2868.092251	23.107994
103.135376	2864.192814	23.113011
103.507204	2862.668584	23.118029
103.610969	2860.134328	23.123047
103.529747	2856.659762	23.128064
103.742177	2857.195145	23.133082
104.078057	2847.007725	23.138099
103.990402	2850.091007	23.143117
103.714303	2852.691278	23.148135
103.795057	2852.180273	23.153152
103.480107	2847.008452	23.158170
103.838046	2844.209658	23.163187
103.959709	2864.934393	23.168205
104.020920	2873.628098	23.173223
104.128124	2878.956066	23.178240
103.971292	2883.548165	23.183258
104.444059	2890.424789	23.188275
104.243961	2894.250373	23.193293
104.754103	2895.516447	23.198311
104.631530	2900.808838	23.203328
105.009808	2907.053820	23.208346
105.091401	2892.518764	23.213363
105.106943	2917.162224	23.218381
105.419107	2924.737159	23.223399
106.078976	2922.025775	23.228416
105.807727	2926.199787	23.233434
105.981914	2921.550547	23.238451
105.779294	2929.194179	23.243469
106.030739	2916.534279	23.248487
106.278454	2926.425971	23.253504
106.180831	2919.740468	23.258522
106.281534	2919.615952	23.263539
106.128458	2922.340366	23.268557
106.109973	2921.695384	23.273575
106.682562	2935.806463	23.278592
106.085666	2949.686739	23.283610
106.730523	2948.042487	23.288627
106.809489	2958.214521	23.293645
106.714413	2952.134144	23.298663
107.064958	2948.113623	23.303680
106.864484	2957.286169	23.308698
106.909551	2967.166554	23.313715
107.454430	2979.264774	23.318733
107.386835	2978.099137	23.323751
107.386036	2981.267285	23.328768
107.368384	2982.230956	23.333786
107.817009	2989.989252	23.338803
107.797581	2992.367902	23.343821
107.793796	3002.293013	23.348839
107.674404	2999.892934	23.353856
107.790302	3005.444328	23.358874
108.004562	3013.735968	23.363891
108.428443	3020.088416	23.368909
108.711092	3034.768893	23.373927
108.843068	3023.931596	23.378944
108.656426	3032.869593	23.383962
108.966570	3020.557401	23.388979
109.131989	3020.269401	23.393997
108.677364	3024.554515	23.399015
109.273829	3015.895629	23.404032
109.385891	3019.927457	23.409050
109.488346	3014.599063	23.414067
109.499892	3030.949361	23.419085
109.477896	3044.871163	23.424103
109.721010	3049.943597	23.429120
109.395254	3050.603528	23.434138
109.610606	3049.274100	23.439155
109.797157	3051.405645	23.444173
109.711662	3060.140675	23.449191
110.103957	3068.442242	23.454208
110.253461	3074.095192	23.459226
110.330982	3075.298252	23.464243
110.351726	3076.117371	23.469261
110.640948	3079.249727	23.474279
111.232108	3096.494769	23.479296
110.994786	3105.689252	23.484314
111.133748	3098.619196	23.489331
111.464890	3094.994799	23.494349
111.560949	3098.084331	23.499367
111.366942	3092.667973	23.504384
111.416375	3097.529161	23.509402
111.599664	3090.259233	23.514419
111.909549	3091.421460	23.519437
111.410975	3099.787069	23.524455
112.129364	3083.697456	23.529472
111.816044	3096.118186	23.534490
112.142478	3104.411778	23.539507
112.097111	3116.755481	23.544525
112.142626	3112.886612	23.549543
112.702848	3112.286373	23.554560
112.650105	3114.441402	23.559578
112.442858	3101.980928	23.564595
112.511125	3114.018782	23.569613
112.788292	3146.262894	23.574631
113.090029	3136.495939	23.579648
113.040064	3140.500682	23.584666
113.073943	3138.956388	23.589683
113.455620	3142.630981	23.594701
113.563185	3147.421137	23.599719
113.701985	3151.760018	23.604736
113.644553	3161.657889	23.609754
113.833370	3156.536822	23.614771
113.893433	3158.366066	23.619789
113.768741	3161.439791	23.624807
114.194920	3154.447759	23.629824
113.834798	3162.523524	23.634842
114.283898	3171.820561	23.639859
114.457447	3186.646422	23.644877
114.312128	3184.620720	23.649895
114.354120	3183.219581	23.654912
114.646308	3194.303013	23.659930
114.495249	3207.671470	23.664947
115.086313	3206.907444	23.669965
115.001990	3204.615317	23.674983
115.261688	3208.488880	23.680000
115.391078	3230.275128	23.685018
115.647853	3235.071318	23.690035
116.342282	3242.874094	23.695053
116.058337	3235.329059	23.700071
116.241436	3236.325656	23.705088
116.027021	3241.414449	23.710106
115.991811	3231.989864	23.715123
116.021213	3232.127175	23.720141
116.047736	3232.800843	23.725159
116.190863	3225.165812	23.730176
116.381754	3235.719929	23.735194
116.674517	3241.155108	23.740211
116.928129	3244.368204	23.745229
116.539172	3256.583452	23.750247
116.784253	3250.401361	23.755264
117.007673	3254.400244	23.760282
117.168707	3248.332078	23.765299
117.357042	3263.399289	23.770317
117.080729	3284.145979	23.775335
117.415836	3276.764600	23.780352
117.402042	3283.679039	23.785370
117.427765	3284.608379	23.790387
117.718341	3288.256748	23.795405
117.678463	3298.340401	23.800423
118.145364	3304.918939	23.805440
118.156641	3303.502006	23.810458
118.207595	3308.613427	23.815475
118.716697	3306.736474	23.820493
118.349746	3325.781119	23.825511
118.936100	3326.434946	23.830528
118.798357	3329.186815	23.835546
118.784828	3331.872839	23.840563
119.089147	3324.589064	23.845581
118.924497	3328.249813	23.850599
119.601154	3335.579151	23.855616
119.691743	3344.731690	23.860634
119.573667	3353.079322	23.865651
120.118016	3344.680488	23.870669
120.013406	3348.887264	23.875687
120.195659	3348.620884	23.880704
119.868877	3349.847592	23.885722
120.086525	3342.189535	23.890739
120.292868	3339.541751	23.895757
120.369611	3365.529472	23.900775
120.539052	3368.731330	23.905792
120.789212	3379.734836	23.910810
120.507812	3373.105946	23.915827
120.925282	3368.811220	23.920845
120.730851	3374.543272	23.925863
120.771735	3381.839296	23.930880
121.304188	3392.745675	23.935898
121.256923	3393.931620	23.940915
121.353059	3396.276235	23.945933
120.987895	3411.967176	23.950951
121.619638	3421.671180	23.955968
121.752641	3426.512334	23.960986
121.794247	3423.785501	23.966003
121.867160	3426.558421	23.971021
122.039791	3452.991486	23.976039
122.452623	3438.829476	23.981056
122.701674	3448.648831	23.986074
122.683191	3450.867927	23.991091
122.953085	3443.136597	23.996109
122.699064	3457.838996	24.001127
123.026775	3453.069682	24.006144
123.242425	3470.766726	24.011162
123.174394	3481.411520	24.016179
123.173016	3473.340004	24.021197
123.535826	3478.530572	24.026215
123.469592	3475.931045	24.031232
123.746635	3470.444836	24.036250
123.733249	3484.073444	24.041267
124.087520	3494.871191	24.046285
123.834910	3508.388228	24.051303
124.127430	3506.239595	24.056320
124.407028	3503.580050	24.061338
124.434519	3500.876014	24.066355
124.520168	3494.557999	24.071373
124.463394	3519.078539	24.076391
124.835821	3512.573257	24.081408
125.163564	3512.545810	24.086426
125.017337	3517.302498	24.091443
125.267453	3509.249175	24.096461
125.340699	3519.493397	24.101479
125.789920	3505.057949	24.106496
125.831180	3512.423271	24.111514
125.653321	3513.447360	24.116531
125.959728	3507.481419	24.121549
125.989880	3502.977916	24.126567
126.242608	3499.899937	24.131584
126.178217	3499.288518	24.136602
126.052000	3519.644879	24.141619
126.484146	3520.561676	24.146637
126.418425	3527.705319	24.151655
126.385392	3527.414730	24.156672
126.677076	3530.365648	24.161690
126.767930	3551.241294	24.166707
126.937713	3542.773645	24.171725
127.256551	3548.272340	24.176743
127.310163	3537.880390	24.181760
127.281691	3544.073274	24.186778
127.270349	3561.620971	24.191795
128.044171	3567.515268	24.196813
128.108775	3575.228765	24.201831
128.013683	3574.256634	24.206848
128.233493	3576.412671	24.211866
128.264117	3581.398004	24.216883
128.325643	3575.599367	24.221901
128.237196	3575.719574	24.226919
128.387800	3588.977381	24.231936
128.676929	3598.357073	24.236954
128.672883	3604.532155	24.241971
129.111090	3606.159458	24.246989
129.036745	3606.278906	24.252007
128.812782	3604.762687	24.257024
128.915610	3609.729775	24.262042
129.132751	3621.352773	24.267059
129.522453	3625.679385	24.272077
129.098923	3639.212626	24.277095
129.530178	3654.564447	24.282112
129.892136	3653.095723	24.287130
129.814304	3664.874690	24.292147
130.639522	3672.639101	24.297165
130.503331	3682.273534	24.302183
130.630949	3679.340265	24.307200
131.201957	3674.928687	24.312218
130.942264	3676.520736	24.317235
130.983641	3671.911376	24.322253
131.360268	3679.154709	24.327271
131.070150	3671.037182	24.332288
131.296924	3669.345138	24.337306
131.156030	3691.844186	24.342323
131.653688	3697.800005	24.347341
131.532359	3694.800455	24.352359
131.612553	3711.423601	24.357376
131.575997	3712.642054	24.362394
131.785117	3725.261861	24.367411
132.390019	3724.035230	24.372429
132.354626	3735.290227	24.377447
132.312471	3735.426397	24.382464
132.395294	3736.905044	24.387482
132.312240	3754.361668	24.392499
132.656746	3758.615474	24.397517
132.728327	3764.052413	24.402535
132.821050	3769.026737	24.407552
133.175320	3776.346267	24.412570
133.293342	3793.377072	24.417587
133.440379	3785.578107	24.422605
133.438795	3786.747463	24.427623
133.674282	3787.803149	24.432640
134.072061	3792.985279	24.437658
134.282334	3808.964862	24.442675
134.350975	3803.230719	24.447693
134.207357	3810.082228	24.452711
134.559613	3807.701982	24.457728
135.058251	3811.231372	24.462746
134.960251	3803.495804	24.467763
135.106581	3800.598790	24.472781
135.129552	3801.237633	24.477799
134.953257	3794.454135	24.482816
135.337619	3792.861201	24.487834
135.311825	3803.923688	24.492851
135.475577	3814.812657	24.497869
135.465300	3826.282489	24.502887
135.502373	3821.181604	24.507904
135.700251	3818.950554	24.512922
135.630602	3840.332358	24.517939
135.761360	3843.170984	24.522957
136.233986	3850.399684	24.527975
136.293267	3852.790240	24.532992
136.494953	3861.375007	24.538010
136.480799	3864.367961	24.543027
136.818699	3874.179569	24.548045
136.932330	3877.774684	24.553063
137.196217	3891.937351	24.558080
137.620137	3900.894459	24.563098
137.453337	3902.682991	24.568115
137.647132	3895.799983	24.573133
138.037637	3895.114812	24.578151
137.954043	3900.629858	24.583168
138.123202	3897.908206	24.588186
138.070715	3895.517780	24.593203
138.184574	3904.191137	24.598221
138.176267	3906.617303	24.603239
138.336482	3913.939101	24.608256
138.553692	3912.400998	24.613274
138.822121	3922.555681	24.618291
138.746789	3936.919452	24.623309
139.055451	3947.028114	24.628327
138.596991	3955.406038	24.633344
139.130782	3958.950118	24.638362
139.468049	3976.105871	24.643379
139.746203	3970.571660	24.648397
139.914532	3974.531025	24.653415
139.571858	3980.644191	24.658432
139.909704	3983.529672	24.663450
140.103434	4006.728606	24.668467
140.283643	3997.473043	24.673485
140.451709	3998.005183	24.678503
140.663985	4005.861792	24.683520
140.959252	4000.869700	24.688538
140.745821	4016.538878	24.693555
141.287947	4025.005553	24.698573
141.138384	4028.099314	24.703591
141.226904	4033.390214	24.708608
141.226653	4020.419861	24.713626
141.499496	4036.967751	24.718643
141.488310	4053.324064	24.723661
141.932177	4048.979109	24.728679
142.008804	4051.240820	24.733696
142.122881	4045.236823	24.738714
142.323957	4072.616369	24.743731
142.485474	4073.188972	24.748749
142.397764	4070.903971	24.753767
142.699342	4066.242360	24.758784
142.886422	4070.180532	24.763802
142.861929	4077.676315	24.768819
142.974946	4085.079247	24.773837
143.682227	4091.125336	24.778855
143.012255	4108.051473	24.783872
143.257297	4101.667449	24.788890
143.551723	4103.059911	24.793907
143.640314	4104.098989	24.798925
143.939874	4113.021682	24.803943
143.677370	4132.237441	24.808960
144.142420	4123.871801	24.813978
144.251925	4126.710059	24.818995
144.734548	4149.765299	24.824013
144.445997	4157.096930	24.829031
144.514863	4157.087144	24.834048
145.042175	4159.952316	24.839066
145.041741	4157.465422	24.844083
145.101733	4166.756206	24.849101
145.477278	4179.195260	24.854119
145.405801	4183.568455	24.859136
145.526616	4176.608023	24.864154
146.142079	4195.811599	24.869171
146.030409	4209.735500	24.874189
146.218745	4211.776346	24.879207
146.176258	4218.467959	24.884224
146.610380	4213.280343	24.889242
146.649197	4212.874680	24.894259
146.584304	4215.882795	24.899277
147.054092	4219.804127	24.904295
146.825160	4240.131176	24.909312
147.307870	4233.086391	24.914330
147.383184	4237.342370	24.919347
147.504125	4236.570297	24.924365
147.261023	4253.171545	24.929383
147.446512	4267.501494	24.934400
148.096692	4262.499389	24.939418
147.953240	4261.427723	24.944435
148.160974	4279.687715	24.949453
148.586842	4286.056895	24.954471
148.269594	4283.279069	24.959488
148.796531	4279.075444	24.964506
148.753619	4277.960355	24.969523
148.636677	4297.796419	24.974541
149.118391	4308.214517	24.979559
149.176554	4314.857219	24.984576
149.443585	4311.687332	24.989594
149.287530	4312.964597	24.994611
149.414947	4325.346406	24.999629
149.518163	4333.574050	25.004647
149.730687	4336.924514	25.009664
149.667238	4352.254183	25.014682
150.301408	4357.011474	25.019699
150.333461	4355.693386	25.024717
150.477349	4357.792012	25.029735
150.297980	4382.114081	25.034752
150.737620	4385.802611	25.039770
150.898726	4387.807823	25.044787
151.327817	4405.409949	25.049805
151.997004	4397.306482	25.054823
151.861965	4409.156906	25.059840
152.028185	4405.965888	25.064858
152.639060	4409.673327	25.069875
152.314331	4410.563492	25.074893
152.478271	4409.551968	25.079911
152.203624	4408.554777	25.084928
152.112293	4405.211876	25.089946
152.529614	4407.003778	25.094963
152.221384	4412.238421	25.099981
152.932538	4424.914287	25.104999
152.560404	4430.333562	25.110016
152.779585	4432.376418	25.115034
153.002939	4431.603919	25.120051
153.034617	4452.382671	25.125069
153.209751	4458.013768	25.130087
153.323158	4467.547900	25.135104
153.649377	4474.539274	25.140122
153.672909	4482.464385	25.145139
153.411278	4499.697418	25.150157
154.349758	4510.174702	25.155175
153.908289	4533.250401	25.160192
154.249595	4520.413675	25.165210
154.752047	4527.504266	25.170227
154.933466	4539.082672	25.175245
155.027807	4539.073393	25.180263
155.128994	4539.057468	25.185280
155.501436	4551.290209	25.190298
155.641004	4559.621423	25.195315
155.678403	4567.907339	25.200333
156.308614	4565.301799	25.205351
156.375397	4568.934757	25.210368
156.437288	4558.769149	25.215386
156.830363	4556.328877	25.220403
156.538452	4556.600907	25.225421
156.677874	4568.504455	25.230439
156.741559	4575.235346	25.235456
156.940380	4578.792106	25.240474
156.859074	4575.404981	25.245491
156.989606	4600.299819	25.250509
157.081848	4604.109706	25.255527
157.516555	4617.374116	25.260544
157.409277	4632.127740	25.265562
157.993584	4633.061159	25.270579
157.866182	4635.726094	25.275597
158.280921	4635.870898	25.280615
158.439562	4640.026561	25.285632
158.785260	4653.559328	25.290650
159.480506	4658.964995	25.295667
159.273427	4661.307628	25.300685
159.274293	4655.893903	25.305703
159.561883	4658.596457	25.310720
159.858496	4660.546982	25.315738
159.616742	4645.895297	25.320755
159.568349	4653.399249	25.325773
160.224463	4675.519285	25.330791
159.960340	4675.463032	25.335808
160.199475	4686.197975	25.340826
160.350811	4679.258257	25.345843
160.471447	4687.415474	25.350861
160.426217	4701.607604	25.355879
160.498324	4716.791541	25.360896
160.610041	4721.239301	25.365914
161.069507	4719.172339	25.370931
161.144365	4742.627521	25.375949
161.088009	4739.708763	25.380967
161.349654	4749.991116	25.385984
161.019939	4770.052013	25.391002
161.756974	4762.551424	25.396019
161.799986	4780.354923	25.401037
162.118083	4789.469461	25.406055
162.368267	4797.503693	25.411072
162.264229	4795.224440	25.416090
162.642325	4813.427710	25.421107
162.605846	4826.322184	25.426125
162.611240	4819.788532	25.431143
163.088094	4839.546662	25.436160
163.323414	4854.634406	25.441178
163.686789	4843.154669	25.446195
163.980023	4852.468674	25.451213
164.232935	4845.210432	25.456231
164.288776	4842.143133	25.461248
163.924379	4843.455720	25.466266
164.525172	4852.618001	25.471283
164.763360	4869.105566	25.476301
165.258682	4864.718009	25.481319
164.968989	4861.129053	25.486336
165.216616	4865.707928	25.491354
165.452447	4861.844531	25.496371
165.412759	4860.143710	25.501389
165.608323	4866.577246	25.506407
165.621232	4858.704268	25.511424
165.588149	4873.150499	25.516442
165.603508	4880.066723	25.521459
165.504676	4889.511026	25.526477
165.702022	4909.991247	25.531495
166.118846	4918.648481	25.536512
166.085320	4923.877192	25.541530
166.375181	4932.247515	25.546547
166.528814	4947.511897	25.551565
166.570230	4970.606738	25.556583
166.916157	4980.471268	25.561600
167.099742	4989.746804	25.566618
167.461958	5000.608860	25.571635
167.611453	5003.963604	25.576653
167.647251	4993.626407	25.581671
168.157806	5018.164443	25.586688
168.084205	5031.643305	25.591706
168.711463	5023.695315	25.596723
168.400569	5031.006634	25.601741
168.910797	5045.199262	25.606759
169.172773	5043.197246	25.611776
169.242308	5047.133861	25.616794
169.464360	5041.031278	25.621811
169.440735	5062.038935	25.626829
169.286570	5066.804097	25.631847
169.670048	5078.154132	25.636864
169.900917	5075.918627	25.641882
170.268367	5094.649297	25.646899
170.635826	5090.879827	25.651917
170.932130	5084.237261	25.656935
170.922361	5088.079118	25.661952
170.857478	5093.291025	25.666970
171.350350	5100.617375	25.671988
171.663773	5121.468503	25.677005
171.746086	5118.326674	25.682023
171.546494	5125.569993	25.687040
171.491461	5119.205310	25.692058
172.029136	5115.112314	25.697076
172.200202	5131.880617	25.702093
171.961796	5136.369920	25.707111
172.230724	5147.925624	25.712128
172.141273	5153.677169	25.717146
172.835344	5173.387947	25.722164
172.727832	5184.017590	25.727181
172.800125	5191.751481	25.732199
173.208869	5199.122520	25.737216
173.235719	5212.232859	25.742234
173.739660	5212.209327	25.747252
173.870436	5215.067103	25.752269
174.049760	5230.491323	25.757287
174.665651	5237.088551	25.762304
174.417551	5238.875727	25.767322
174.568325	5235.038134	25.772340
174.350885	5235.666431	25.777357
174.763853	5256.260259	25.782375
175.227319	5257.920187	25.787392
175.125839	5256.535921	25.792410
175.460544	5266.523778	25.797428
175.255156	5256.068034	25.802445
175.257017	5275.142184	25.807463
175.783031	5270.233571	25.812480
175.668897	5279.729470	25.817498
176.080248	5284.276639	25.822516
175.997405	5296.601088	25.827533
176.264866	5314.375909	25.832551
176.538373	5311.507972	25.837568
176.941142	5334.165483	25.842586
177.029927	5335.895324	25.847604
177.309161	5339.662620	25.852621
177.295642	5339.616068	25.857639
177.521571	5351.579134	25.862656
177.194436	5370.077796	25.867674
177.920720	5373.550567	25.872692
177.833554	5383.490988	25.877709
177.796430	5397.039732	25.882727
178.340122	5398.852575	25.887744
178.054802	5420.819997	25.892762
178.561711	5426.210647	25.897780
178.963417	5429.433156	25.902797
179.049267	5458.897677	25.907815
179.632458	5457.171646	25.912832
179.580202	5454.889236	25.917850
180.028094	5457.518138	25.922868
180.243126	5464.306263	25.927885
179.962401	5479.148462	25.932903
180.707146	5485.609476	25.937920
180.466267	5483.779650	25.942938
180.681189	5473.031292	25.947956
180.850299	5492.300905	25.952973
180.931554	5498.903268	25.957991
180.955378	5509.742152	25.963008
181.325844	5514.531647	25.968026
181.613763	5539.282988	25.973044
181.768702	5542.542435	25.978061
181.931497	5531.986176	25.983079
182.188301	5533.544093	25.988096
182.158331	5555.233151	25.993114
182.583755	5566.075685	25.998132
182.793189	5562.530740	26.003149
182.807521	5565.900891	26.008167
183.417884	5575.021060	26.013184
183.156207	5575.988271	26.018202
183.364808	5582.477438	26.023220
183.360703	5573.749227	26.028237
183.657018	5602.533346	26.033255
183.928309	5607.666141	26.038272
183.916272	5612.870258	26.043290
184.394798	5617.748222	26.048308
184.705804	5626.031143	26.053325
184.697211	5629.045958	26.058343
184.915338	5631.792475	26.063360
184.889917	5646.748510	26.068378
185.256898	5662.891095	26.073396
185.446173	5660.387523	26.078413
185.454788	5666.998044	26.083431
185.979890	5669.740217	26.088448
185.686269	5682.573996	26.093466
185.996766	5679.668365	26.098484
186.416931	5685.575169	26.103501
186.087600	5698.123459	26.108519
186.593295	5708.421960	26.113536
186.678246	5715.330179	26.118554
186.782401	5724.721687	26.123572
187.409813	5741.050432	26.128589
187.189435	5750.890271	26.133607
187.416254	5731.858891	26.138624
187.331069	5758.570469	26.143642
187.510527	5763.766562	26.148660
187.803080	5778.324323	26.153677
188.015516	5789.540943	26.158695
188.484694	5790.417892	26.163712
188.651427	5796.234374	26.168730
188.901446	5808.567913	26.173748
188.975210	5819.028566	26.178765
189.132770	5833.960000	26.183783
189.285395	5834.355357	26.188800
189.349051	5844.500293	26.193818
190.009245	5851.529936	26.198836
190.159819	5853.918286	26.203853
189.990807	5856.107507	26.208871
190.503884	5875.337186	26.213888
190.471673	5874.579363	26.218906
190.686616	5886.468256	26.223924
190.871521	5885.490976	26.228941
190.787888	5905.541715	26.233959
191.381432	5902.228461	26.238976
191.420403	5932.071016	26.243994
191.592996	5935.074010	26.249012
192.103683	5938.632224	26.254029
191.994780	5957.412851	26.259047
192.213735	5966.575205	26.264064
192.244736	5966.224349	26.269082
192.378088	5987.850733	26.274100
193.125182	5993.870506	26.279117
192.636663	6004.181780	26.284135
193.266078	5998.050774	26.289152
193.434706	6014.241521	26.294170
193.274028	6023.418710	26.299188
193.478285	6035.713533	26.304205
193.974429	6055.412506	26.309223
194.232888	6063.425540	26.314240
194.175249	6072.321846	26.319258
194.520843	6081.662570	26.324276
195.228103	6090.626804	26.329293
194.655344	6108.295091	26.334311
195.523866	6097.834284	26.339328
195.518169	6112.413373	26.344346
196.012836	6110.591664	26.349364
196.091733	6125.564751	26.354381
196.204819	6135.312605	26.359399
196.446519	6131.236847	26.364416
196.665643	6131.380191	26.369434
196.629536	6131.578388	26.374452
196.652856	6160.254343	26.379469
196.500748	6170.319427	26.384487
197.151030	6172.470727	26.389504
197.216628	6187.175917	26.394522
197.198955	6195.653748	26.399540
197.604551	6213.468939	26.404557
197.611077	6228.987328	26.409575
197.707325	6228.519335	26.414592
198.105567	6244.079222	26.419610
198.234538	6260.387842	26.424628
198.737028	6270.335173	26.429645
198.730075	6282.828193	26.434663
199.143619	6294.349774	26.439680
199.539697	6306.973002	26.444698
199.453148	6310.220602	26.449716
199.911844	6309.800511	26.454733
199.890644	6330.960679	26.459751
200.041287	6342.987370	26.464768
200.010362	6343.629726	26.469786
200.491535	6350.311166	26.474804
200.535340	6359.913101	26.479821
200.590731	6374.613066	26.484839
200.926398	6371.259707	26.489856
201.187186	6395.379685	26.494874
201.377515	6399.920450	26.499892
201.480965	6398.910942	26.504909
201.664674	6419.543457	26.509927
201.907958	6421.853536	26.514944
201.997144	6430.652487	26.519962
202.130634	6450.806595	26.524980
202.515225	6458.832819	26.529997
202.364222	6472.958985	26.535015
202.771387	6485.065403	26.540032
203.112467	6491.384150	26.545050
203.309686	6513.084169	26.550068
203.823369	6517.581679	26.555085
203.876829	6518.299075	26.560103
203.966529	6532.861972	26.565120
204.319428	6535.951016	26.570138
204.354660	6550.728521	26.575156
204.797225	6560.732427	26.580173
205.018878	6563.442293	26.585191
205.522104	6568.157364	26.590208
205.643018	6585.038695	26.595226
205.719750	6585.751455	26.600244
205.946046	6595.465099	26.605261
205.900876	6599.502219	26.610279
206.408865	6614.552812	26.615296
206.332083	6621.980482	26.620314
206.505513	6626.928962	26.625332
206.875963	6629.436198	26.630349
206.895225	6649.429098	26.635367
206.932385	6660.966784	26.640384
207.506588	6673.805778	26.645402
207.302478	6687.990548	26.650420
207.543649	6687.612761	26.655437
207.527643	6716.374997	26.660455
207.986438	6717.912200	26.665472
208.166981	6741.759284	26.670490
208.255365	6750.182834	26.675508
208.706618	6759.322159	26.680525
208.840375	6780.677030	26.685543
209.201000	6784.039737	26.690560
209.480421	6795.902889	26.695578
209.671326	6801.659030	26.700596
209.963534	6823.500493	26.705613
209.784208	6830.280451	26.710631
210.235569	6833.679347	26.715648
210.550443	6849.096888	26.720666
210.482684	6865.981396	26.725684
211.472285	6868.250699	26.730701
211.256173	6890.882146	26.735719
211.469738	6884.323420	26.740736
211.584047	6878.356120	26.745754
211.617023	6905.169005	26.750772
211.885924	6910.963472	26.755789
212.148784	6922.400184	26.760807
212.603589	6944.360615	26.765824
212.993603	6947.876026	26.770842
212.770202	6945.495706	26.775860
213.352790	6958.262655	26.780877
213.879710	6967.158789	26.785895
213.512684	6975.480623	26.790912
213.422059	6976.120284	26.795930
214.029576	6988.608235	26.800948
214.443849	6990.151262	26.805965
214.214603	6995.984902	26.810983
214.527689	7004.552554	26.816000
215.039884	7017.419422	26.821018
214.859632	7024.795881	26.826036
214.785894	7034.145937	26.831053
214.718556	7047.678251	26.836071
215.224894	7058.890442	26.841088
215.598776	7072.660079	26.846106
215.530125	7092.169493	26.851124
216.302171	7104.412116	26.856141
216.293921	7125.252978	26.861159
216.530930	7122.425420	26.866176
216.893495	7125.907607	26.871194
217.059998	7141.528796	26.876212
217.221317	7147.615270	26.881229
217.345284	7168.340569	26.886247
217.592064	7169.854627	26.891264
218.004119	7179.876581	26.896282
218.329530	7206.473002	26.901300
218.472700	7206.717152	26.906317
218.477937	7209.834739	26.911335
218.862249	7239.559572	26.916352
219.145845	7239.697770	26.921370
219.130794	7246.753180	26.926388
219.393506	7262.579899	26.931405
219.560072	7265.187943	26.936423
219.793261	7291.128669	26.941440
220.319504	7295.339185	26.946458
220.483174	7298.506968	26.951476
221.057635	7318.045681	26.956493
220.970872	7325.749444	26.961511
221.240958	7318.763712	26.966528
221.218912	7329.397184	26.971546
221.209247	7353.976925	26.976564
221.878143	7355.991410	26.981581
222.219005	7383.280307	26.986599
221.910825	7390.956953	26.991616
222.357400	7397.349973	26.996634
222.330309	7404.459433	27.001652
222.463481	7409.488866	27.006669
222.755909	7433.745395	27.011687
222.708681	7440.096509	27.016704
223.352310	7461.578205	27.021722
223.433274	7476.791682	27.026740
224.134602	7488.550065	27.031757
224.206510	7497.222499	27.036775
224.446136	7517.570707	27.041792
224.734274	7521.689944	27.046810
224.713471	7532.194164	27.051828
225.060434	7545.621296	27.056845
225.068080	7561.681947	27.061863
225.280192	7568.198921	27.066880
225.737516	7577.144731	27.071898
225.762653	7586.487408	27.076916
226.257045	7607.714374	27.081933
226.598710	7613.698706	27.086951
226.538855	7621.152396	27.091968
227.224551	7640.182357	27.096986
227.356848	7644.788227	27.102004
227.510771	7652.684677	27.107021
227.861807	7672.234818	27.112039
227.911955	7679.259146	27.117056
228.217187	7672.324944	27.122074
228.345153	7686.684851	27.127092
228.649486	7706.481439	27.132109
228.651491	7695.511613	27.137127
228.679785	7716.024241	27.142144
229.104028	7731.233912	27.147162
228.987451	7740.548938	27.152180
229.411600	7750.636207	27.157197
229.794395	7763.714153	27.162215
229.678182	7775.667163	27.167232
230.075660	7783.410718	27.172250
230.348366	7800.875536	27.177268
230.604243	7821.663347	27.182285
231.001956	7826.979958	27.187303
231.205917	7824.798943	27.192320
231.339653	7840.311237	27.197338
231.453919	7864.582950	27.202356
231.675752	7859.575820	27.207373
231.867731	7878.741361	27.212391
231.701134	7891.247105	27.217408
232.076894	7900.153824	27.222426
232.695773	7921.060484	27.227444
232.866472	7932.265052	27.232461
233.378572	7948.553734	27.237479
233.358136	7967.117283	27.242496
233.749266	7972.207383	27.247514
233.624603	7982.918932	27.252532
234.008113	7996.045002	27.257549
234.497555	8005.985351	27.262567
234.372341	8033.646335	27.267584
234.891658	8032.147244	27.272602
234.965348	8050.732331	27.277620
235.421625	8070.240333	27.282637
235.923337	8074.360596	27.287655
236.031500	8092.409102	27.292672
235.979878	8106.688048	27.297690
236.292509	8119.678650	27.302708
236.764712	8128.464765	27.307725
236.802893	8132.245856	27.312743
236.757695	8146.045625	27.317760
237.169949	8154.243009	27.322778
237.254226	8165.404543	27.327796
237.422080	8191.137776	27.332813
237.780106	8198.854194	27.337831
237.991105	8221.442820	27.342848
238.239605	8230.928502	27.347866
238.404331	8248.799248	27.352884
238.599030	8259.228099	27.357901
239.201475	8278.905943	27.362919
239.150436	8296.289406	27.367936
239.678664	8314.658555	27.372954
239.642434	8325.559716	27.377972
239.804704	8349.387028	27.382989
240.401766	8348.029435	27.388007
240.528748	8373.148993	27.393024
241.027959	8364.966909	27.398042
241.034825	8388.912957	27.403060
241.441612	8399.027145	27.408077
241.828457	8408.564080	27.413095
242.011383	8421.840291	27.418112
242.084925	8432.518543	27.423130
242.556337	8443.965156	27.428148
242.689927	8462.745619	27.433165
243.241081	8458.042999	27.438183
243.045029	8464.422307	27.443200
243.539467	8473.375085	27.448218
243.558800	8488.803755	27.453236
243.728358	8495.052445	27.458253
243.867873	8512.196636	27.463271
244.068197	8531.506524	27.468288
244.312251	8543.276007	27.473306
244.427552	8557.060591	27.478324
244.805945	8574.786836	27.483341
245.154858	8581.495848	27.488359
244.881895	8596.062372	27.493376
245.118308	8616.221093	27.498394
245.353528	8637.867305	27.503412
245.892506	8647.955832	27.508429
246.176972	8660.887730	27.513447
246.205829	8678.479740	27.518464
246.530026	8698.389284	27.523482
247.100591	8709.770836	27.528500
247.423640	8725.358212	27.533517
248.015088	8725.048442	27.538535
247.894314	8734.479752	27.543552
248.154436	8733.719878	27.548570
248.421094	8757.364303	27.553588
248.396508	8756.524728	27.558605
248.718096	8778.478238	27.563623
248.987381	8796.707260	27.568640
249.444579	8818.071980	27.573658
249.790491	8832.693826	27.578676
249.838570	8830.896910	27.583693
250.074987	8848.026996	27.588711
250.204805	8858.810442	27.593728
250.373534	8872.708557	27.598746
250.893224	8877.741433	27.603764
251.207005	8907.862331	27.608781
251.590227	8914.785591	27.613799
251.714119	8928.805402	27.618816
252.078038	8939.767574	27.623834
252.160885	8950.554130	27.628852
252.367615	8963.684267	27.633869
252.501532	8980.706208	27.638887
252.885319	8987.895670	27.643904
253.009653	9000.929189	27.648922
253.483312	9007.902116	27.653940
253.578503	9038.602215	27.658957
254.127221	9037.167494	27.663975
254.225893	9065.148482	27.668992
254.162817	9067.414345	27.674010
254.247895	9081.525793	27.679028
254.265265	9107.431148	27.684045
255.048396	9123.580063	27.689063
255.371249	9144.594054	27.694080
255.371583	9157.217314	27.699098
256.249436	9170.916378	27.704116
256.110064	9190.007571	27.709133
256.509056	9188.853648	27.714151
256.740330	9218.099390	27.719168
257.135639	9221.410404	27.724186
257.551557	9237.378372	27.729204
257.641355	9259.181843	27.734221
257.827945	9252.413130	27.739239
257.905027	9275.610732	27.744256
257.860106	9289.780908	27.749274
258.218808	9311.061756	27.754292
258.420979	9329.356065	27.759309
259.011505	9334.810642	27.764327
259.226385	9347.733346	27.769344
259.525877	9363.784523	27.774362
259.828072	9375.262181	27.779380
259.925982	9399.138735	27.784397
260.456214	9404.679733	27.789415
260.693059	9427.090108	27.794432
261.014424	9427.558467	27.799450
261.179959	9451.419178	27.804468
261.034058	9469.227689	27.809485
261.539235	9471.088370	27.814503
261.619782	9497.177692	27.819520
261.871055	9508.421235	27.824538
262.641288	9523.263384	27.829556
262.548294	9534.951525	27.834573
263.104281	9542.813082	27.839591
263.474086	9555.906470	27.844608
263.307784	9550.526628	27.849626
263.708483	9575.215957	27.854644
263.620385	9587.303526	27.859661
264.313158	9591.540669	27.864679
264.591194	9612.987315	27.869696
264.666436	9616.477440	27.874714
264.978020	9637.361595	27.879732
265.208322	9655.175789	27.884749
265.797069	9663.841052	27.889767
265.841600	9678.757778	27.894784
265.858994	9683.565240	27.899802
266.476382	9702.138663	27.904820
266.352678	9713.757177	27.909837
266.515330	9728.590585	27.914855
266.708530	9741.662939	27.919872
267.051666	9769.323443	27.924890
267.443070	9784.493244	27.929908
267.551773	9796.650808	27.934925
267.968556	9818.690039	27.939943
268.465715	9835.125718	27.944960
268.502136	9853.713552	27.949978
269.180265	9867.880361	27.954996
269.187488	9890.973033	27.960013
269.423759	9892.410318	27.965031
269.798781	9915.494139	27.970048
270.093270	9931.015728	27.975066
270.315049	9934.625049	27.980084
270.661469	9949.822148	27.985101
271.221852	9969.097805	27.990119
271.328928	9979.257883	27.995136
271.797898	10000.117245	28.000154
272.180444	10005.905064	28.005172
272.252308	10018.348569	28.010189
272.115743	10037.158263	28.015207
272.484548	10043.499842	28.020224
272.757753	10066.543223	28.025242
273.101795	10074.179359	28.030260
273.453386	10098.625521	28.035277
273.474067	10108.507700	28.040295
273.794826	10121.422169	28.045312
274.010020	10142.675879	28.050330
274.587571	10155.268192	28.055348
274.669752	10172.828590	28.060365
275.244159	10187.473729	28.065383
275.284051	10202.082881	28.070400
275.342650	10228.563056	28.075418
275.793077	10232.693166	28.080436
275.836571	10258.120991	28.085453
276.255362	10269.490179	28.090471
276.512539	10297.837052	28.095488
276.788424	10303.105335	28.100506
277.406091	10319.245824	28.105524
277.624777	10335.854953	28.110541
277.740291	10349.514202	28.115559
278.141952	10361.469287	28.120576
277.986767	10384.706147	28.125594
278.795198	10394.133522	28.130612
278.840171	10413.494239	28.135629
279.318894	10419.290712	28.140647
279.827734	10432.123089	28.145664
279.861142	10441.715806	28.150682
280.260399	10460.355367	28.155700
280.615224	10473.381867	28.160717
281.113400	10476.205781	28.165735
281.066766	10492.167267	28.170752
280.929962	10503.987053	28.175770
281.462109	10507.687729	28.180788
281.640607	10524.230436	28.185805
281.862905	10536.812523	28.190823
282.183772	10529.958022	28.195840
282.371852	10562.785431	28.200858
282.561293	10568.335977	28.205876
282.767649	10587.359781	28.210893
283.252944	10606.038055	28.215911
283.560589	10619.060666	28.220928
283.417231	10645.916881	28.225946
283.837686	10664.528746	28.230964
284.010797	10685.568755	28.235981
284.279014	10703.112331	28.240999
284.645941	10719.522416	28.246016
285.064477	10754.454233	28.251034
285.371998	10760.328016	28.256052
285.514382	10792.015555	28.261069
286.095140	10807.630846	28.266087
286.529425	10814.397576	28.271104
286.693308	10833.622513	28.276122
287.484651	10852.407987	28.281140
287.343052	10859.196000	28.286157
287.119853	10878.061194	28.291175
287.804078	10901.783839	28.296192
287.876140	10918.728256	28.301210
288.405632	10938.296185	28.306228
288.389133	10958.709283	28.311245
288.808139	10969.802393	28.316263
289.379523	10993.413066	28.321280
289.280628	11008.754998	28.326298
289.826179	11040.705619	28.331316
290.042261	11051.711043	28.336333
290.588934	11070.474241	28.341351
290.842595	11088.702940	28.346368
290.978331	11112.756195	28.351386
291.253044	11130.530795	28.356404
291.553317	11144.212135	28.361421
291.817119	11160.006291	28.366439
292.474881	11175.494164	28.371456
292.488689	11201.860442	28.376474
292.786349	11205.140766	28.381492
293.031420	11232.400081	28.386509
293.501762	11244.732878	28.391527
293.512587	11261.574336	28.396544
293.839448	11284.455367	28.401562
294.593996	11298.712432	28.406580
294.701423	11315.227532	28.411597
294.932820	11335.278619	28.416615
295.251051	11346.021517	28.421632
295.509031	11366.815153	28.426650
295.817534	11390.704710	28.431668
295.875874	11397.480339	28.436685
296.096016	11430.278205	28.441703
296.578725	11439.689205	28.446720
296.843737	11455.258114	28.451738
297.374866	11470.953175	28.456756
297.866883	11486.697270	28.461773
297.878264	11509.559929	28.466791
298.471700	11510.022719	28.471808
298.437991	11528.739121	28.476826
298.735552	11540.007154	28.481844
298.982702	11570.834261	28.486861
299.311965	11589.615141	28.491879
299.565390	11605.030110	28.496896
299.760458	11625.388545	28.501914
299.788877	11640.951096	28.506932
300.318758	11671.960088	28.511949
300.592997	11685.688743	28.516967
301.251400	11689.405831	28.521984
301.330942	11713.062726	28.527002
301.900298	11732.631325	28.532020
302.012864	11746.475037	28.537037
302.314818	11762.269770	28.542055
302.945321	11774.590647	28.547072
303.099259	11787.203147	28.552090
302.898177	11801.417132	28.557108
303.346134	11826.960908	28.562125
303.396560	11848.446629	28.567143
303.881059	11851.347907	28.572160
303.678979	11877.766776	28.577178
304.290492	11899.076175	28.582196
304.591147	11930.892602	28.587213
304.614137	11942.392309	28.592231
305.251979	11975.051228	28.597248
305.521970	12000.177201	28.602266
305.791515	12018.158489	28.607284
306.198018	12033.898363	28.612301
306.671186	12064.993135	28.617319
307.061012	12086.051098	28.622336
307.154546	12106.710593	28.627354
307.796660	12130.358499	28.632372
308.230639	12147.731231	28.637389
308.410908	12167.065348	28.642407
308.530625	12181.095772	28.647424
308.861354	12203.909703	28.652442
309.317868	12226.091417	28.657460
309.568651	12237.074571	28.662477
309.786429	12266.459659	28.667495
310.481264	12289.736627	28.672512
310.396468	12302.214123	28.677530
310.625306	12325.218432	28.682548
311.054879	12342.576344	28.687565
311.172052	12367.327912	28.692583
311.778393	12393.802914	28.697600
311.612763	12416.860038	28.702618
312.237156	12438.333482	28.707636
312.775446	12452.194004	28.712653
312.617324	12480.793880	28.717671
313.101224	12499.807088	28.722688
313.441711	12523.973528	28.727706
313.573306	12544.275860	28.732724
314.302290	12570.428282	28.737741
314.664814	12590.900465	28.742759
315.054557	12614.986398	28.747776
315.250617	12641.375276	28.752794
315.766735	12657.877678	28.757812
316.088588	12672.773325	28.762829
316.505454	12694.719557	28.767847
316.831105	12709.289976	28.772864
317.403254	12734.288279	28.777882
317.088095	12741.419406	28.782900
317.650795	12760.782334	28.787917
317.659625	12785.120673	28.792935
317.691153	12797.733733	28.797952
318.009146	12832.691405	28.802970
318.494843	12865.768126	28.807988
319.066026	12879.309964	28.813005
319.249517	12893.141338	28.818023
319.508199	12919.636919	28.823040
319.534074	12943.211508	28.828058
320.092905	12964.776874	28.833076
320.681958	12986.209617	28.838093
320.723667	13020.115004	28.843111
321.056926	13030.355393	28.848128
321.324025	13057.350949	28.853146
321.160177	13069.233808	28.858164
322.051994	13085.458560	28.863181
322.021045	13119.784346	28.868199
322.599700	13139.102535	28.873216
322.853914	13170.300277	28.878234
323.262170	13187.758754	28.883252
323.758952	13206.460199	28.888269
323.717394	13234.829351	28.893287
324.398150	13249.517986	28.898304
324.753076	13265.094239	28.903322
325.023022	13292.893447	28.908340
325.456105	13306.746900	28.913357
325.301254	13328.618412	28.918375
325.968624	13353.061354	28.923392
326.205121	13373.117266	28.928410
326.571180	13397.852845	28.933428
327.071515	13416.612254	28.938445
327.220761	13440.360984	28.943463
327.443583	13453.202922	28.948480
327.606021	13485.220199	28.953498
327.880433	13510.571561	28.958516
328.326281	13534.788255	28.963533
328.349283	13564.635012	28.968551
329.173247	13592.571550	28.973568
329.639510	13619.068583	28.978586
329.792068	13651.212323	28.983604
330.047283	13664.627452	28.988621
330.546926	13698.341831	28.993639
330.815202	13724.217768	28.998656
331.254887	13744.376042	29.003674
331.321892	13773.802987	29.008692
331.875377	13799.381255	29.013709
331.958211	13822.068277	29.018727
332.561520	13836.973567	29.023744
333.409788	13859.729377	29.028762
333.745521	13872.327589	29.033780
334.020620	13891.066512	29.038797
333.975093	13913.473889	29.043815
334.403285	13939.883184	29.048832
334.684294	13955.576349	29.053850
334.609106	13980.939023	29.058868
335.712586	14002.253291	29.063885
335.701428	14026.705533	29.068903
336.050865	14055.107530	29.073920
336.280594	14067.561108	29.078938
336.657531	14101.074407	29.083956
337.023524	14117.644118	29.088973
337.513709	14152.311344	29.093991
337.427795	14170.615465	29.099008
337.735951	14197.231015	29.104026
338.189183	14229.619269	29.109044
338.733086	14242.769600	29.114061
339.050740	14277.030659	29.119079
338.767048	14301.080821	29.124096
339.236325	14331.832261	29.129114
339.789553	14367.420954	29.134132
340.149817	14384.858713	29.139149
340.551564	14416.877605	29.144167
340.967828	14444.782216	29.149184
341.475359	14468.034993	29.154202
341.760261	14482.957326	29.159220
342.342525	14505.378234	29.164237
342.701860	14533.810945	29.169255
343.008861	14552.773877	29.174272
343.522381	14563.128818	29.179290
343.621195	14584.605404	29.184308
344.247185	14601.452516	29.189325
344.350358	14615.527174	29.194343
344.558490	14628.949313	29.199360
344.807682	14652.325489	29.204378
345.102148	14673.043236	29.209396
345.575667	14683.666505	29.214413
345.519101	14715.292163	29.219431
345.981754	14744.297596	29.224448
346.227181	14758.374049	29.229466
346.228358	14793.516015	29.234484
346.674085	14821.665415	29.239501
347.053389	14855.302801	29.244519
346.951964	14877.942975	29.249536
347.248879	14909.962845	29.254554
347.610036	14959.443308	29.259572
348.086725	14989.064685	29.264589
348.678129	15017.948421	29.269607
349.220548	15048.090176	29.274624
349.788171	15075.810047	29.279642
350.358042	15103.959874	29.284660
350.454570	15127.948313	29.289677
350.865330	15161.038932	29.294695
351.137180	15182.511302	29.299712
351.812956	15202.205168	29.304730
351.678893	15237.091488	29.309748
352.196067	15262.069666	29.314765
352.763812	15281.160508	29.319783
353.275549	15307.197245	29.324800
353.521368	15335.066959	29.329818
353.679018	15362.248351	29.334836
354.596862	15381.300280	29.339853
354.794538	15408.032225	29.344871
355.204759	15432.854988	29.349888
355.474708	15439.975550	29.354906
355.657522	15474.058101	29.359924
356.139763	15505.362828	29.364941
356.175383	15518.497438	29.369959
356.879644	15548.712626	29.374976
357.041250	15564.795918	29.379994
357.171577	15599.052911	29.385012
357.947227	15624.893584	29.390029
358.370615	15650.217295	29.395047
358.374025	15668.725810	29.400064
358.710670	15691.198450	29.405082
358.738050	15732.625463	29.410100
359.512129	15762.935094	29.415117
360.087930	15788.857963	29.420135
360.298309	15813.758509	29.425152
360.661386	15841.215626	29.430170
361.230813	15861.315629	29.435188
361.710333	15886.389256	29.440205
361.582772	15914.287070	29.445223
361.976192	15942.719731	29.450240
362.431035	15959.680107	29.455258
362.649806	15995.021900	29.460276
363.429276	16019.904228	29.465293
363.351610	16056.510472	29.470311
363.896072	16089.700623	29.475328
364.260545	16116.492803	29.480346
364.264527	16141.000847	29.485364
364.880552	16158.220048	29.490381
365.002943	16191.418786	29.495399
365.162620	16226.085194	29.500416
366.169410	16257.851489	29.505434
366.357637	16295.569635	29.510452
366.412964	16319.725826	29.515469
366.946912	16354.811314	29.520487
367.234388	16379.796105	29.525504
367.635520	16411.574666	29.530522
367.892712	16430.708785	29.535540
368.496990	16455.048588	29.540557
368.647621	16482.669609	29.545575
369.280599	16513.667579	29.550592
369.644619	16533.980517	29.555610
369.928068	16560.443203	29.560628
370.421658	16586.434527	29.565645
370.818118	16612.848644	29.570663
370.848596	16643.520982	29.575680
371.409410	16660.596949	29.580698
371.797349	16695.614326	29.585716
372.077127	16699.061087	29.590733
372.533390	16730.042999	29.595751
372.772833	16766.182192	29.600768
373.473009	16780.820355	29.605786
373.753284	16813.220255	29.610804
374.319068	16830.766886	29.615821
374.653197	16859.338617	29.620839
374.619767	16888.477220	29.625856
375.109626	16915.033992	29.630874
375.628303	16959.089265	29.635892
375.771611	16979.612673	29.640909
376.192271	17012.815711	29.645927
376.747011	17043.594331	29.650944
376.894571	17065.661924	29.655962
377.249055	17098.691658	29.660980
377.670374	17131.700939	29.665997
377.830063	17152.797205	29.671015
378.478648	17201.402947	29.676032
378.912126	17242.342496	29.681050
379.627894	17262.460975	29.686068
379.419602	17289.220590	29.691085
380.136373	17322.833955	29.696103
380.371102	17359.746049	29.701120
380.888678	17381.224750	29.706138
381.264148	17422.874240	29.711156
381.622563	17453.476461	29.716173
382.023315	17482.533214	29.721191
382.584702	17512.055254	29.726208
383.049865	17546.044901	29.731226
383.275410	17576.279978	29.736244
383.738616	17593.756120	29.741261
384.327845	17616.394504	29.746279
384.449685	17645.024792	29.751296
385.003385	17670.557031	29.756314
385.275208	17697.909376	29.761332
385.598715	17726.481207	29.766349
385.984254	17755.287159	29.771367
386.171089	17795.952041	29.776384
386.910515	17816.844435	29.781402
387.438372	17846.891251	29.786420
387.657703	17872.018833	29.791437
387.759506	17893.801891	29.796455
388.240678	17934.062134	29.801472
388.694384	17958.129556	29.806490
388.917266	17983.467956	29.811508
389.516396	18021.796720	29.816525
389.864065	18053.218400	29.821543
390.087325	18090.764577	29.826560
390.724457	18117.194858	29.831578
390.787129	18148.444763	29.836596
391.360123	18175.120638	29.841613
391.723338	18208.067583	29.846631
392.286664	18240.133361	29.851648
392.539850	18261.726322	29.856666
392.620735	18304.189761	29.861684
393.244373	18323.293795	29.866701
393.750976	18351.718165	29.871719
394.119834	18392.732723	29.876736
394.642047	18414.759019	29.881754
394.741720	18430.194816	29.886772
395.057522	18457.695622	29.891789
395.474751	18491.863815	29.896807
395.630597	18523.762686	29.901824
395.943439	18552.716048	29.906842
396.622731	18587.649786	29.911860
396.954668	18619.776660	29.916877
397.504153	18644.734111	29.921895
397.701549	18680.917529	29.926912
398.302198	18707.572340	29.931930
398.549137	18746.791858	29.936948
399.052536	18789.360018	29.941965
399.403297	18813.414184	29.946983
399.813724	18847.365101	29.952000
400.261891	18868.694836	29.957018
400.782525	18910.552613	29.962036
401.388351	18953.656011	29.967053
401.654908	18969.227065	29.972071
401.855894	19001.098883	29.977088
402.336868	19024.636785	29.982106
402.706110	19070.850652	29.987124
402.809757	19092.092652	29.992141
403.543648	19122.126590	29.997159
403.994361	19159.897652	30.002176
404.612137	19193.061385	30.007194
404.866392	19234.147425	30.012212
405.074573	19257.839582	30.017229
405.403700	19292.334567	30.022247
405.722565	19335.989351	30.027264
406.363378	19370.513318	30.032282
406.550824	19404.063993	30.037300
407.098101	19442.478702	30.042317
407.826997	19466.534292	30.047335
408.121097	19507.790980	30.052352
408.881549	19527.644684	30.057370
409.605880	19562.301844	30.062388
409.617364	19587.751762	30.067405
410.158382	19616.659746	30.072423
410.559220	19644.577256	30.077440
410.682375	19666.937686	30.082458
411.328476	19701.625424	30.087476
411.349669	19733.766450	30.092493
411.960924	19766.790511	30.097511
412.256966	19804.317454	30.102528
412.763840	19830.188681	30.107546
413.115974	19854.125875	30.112564
413.260093	19897.114195	30.117581
413.937324	19931.609645	30.122599
414.366516	19970.570109	30.127616
414.787096	19997.982010	30.132634
415.293517	20031.578900	30.137652
415.627900	20069.962488	30.142669
416.335718	20090.233911	30.147687
416.263756	20128.713258	30.152704
416.979521	20150.205303	30.157722
417.679019	20179.898406	30.162740
417.798783	20212.995224	30.167757
418.322656	20235.816683	30.172775
418.488041	20273.585447	30.177792
419.324827	20304.679733	30.182810
419.508979	20329.509390	30.187828
419.723364	20361.402072	30.192845
420.257419	20392.286477	30.197863
420.518280	20426.120297	30.202880
421.011990	20463.828846	30.207898
421.547364	20497.035603	30.212916
421.546368	20518.394477	30.217933
422.013441	20554.619294	30.222951
422.427323	20586.460468	30.227968
422.400724	20616.422710	30.232986
423.044355	20649.654422	30.238004
423.633615	20683.008716	30.243021
424.155682	20716.902376	30.248039
424.287640	20750.859086	30.253056
424.461909	20789.234549	30.258074
425.088800	20818.131971	30.263092
424.963525	20872.692779	30.268109
425.996728	20905.899944	30.273127
426.768911	20956.187929	30.278144
426.989871	20990.113048	30.283162
427.746032	21023.471931	30.288180
427.991001	21060.638033	30.293197
428.794939	21085.350470	30.298215
429.094680	21123.393745	30.303232
429.510093	21158.374941	30.308250
430.110945	21185.063622	30.313268
430.513466	21217.377725	30.318285
431.248505	21232.127573	30.323303
431.637776	21262.318560	30.328320
432.163339	21283.129288	30.333338
432.397070	21308.418889	30.338356
432.673541	21345.470035	30.343373
433.352051	21376.236162	30.348391
433.542802	21404.990758	30.353408
434.244536	21431.245305	30.358426
434.526467	21462.424097	30.363444
434.865433	21493.289200	30.368461
435.271197	21523.742816	30.373479
435.527722	21556.677733	30.378496
436.022805	21603.719713	30.383514
436.509867	21632.726817	30.388532
436.846921	21666.495331	30.393549
437.568682	21696.613151	30.398567
437.715348	21738.975046	30.403584
438.238998	21768.785203	30.408602
438.586468	21790.450670	30.413620
439.062772	21830.178674	30.418637
439.543851	21869.221665	30.423655
439.831503	21902.131606	30.428672
440.581785	21941.614282	30.433690
441.005619	21965.799628	30.438708
441.196758	22009.796259	30.443725
441.890035	22041.567138	30.448743
442.542931	22076.854674	30.453760
442.504259	22109.134696	30.458778
443.172428	22137.581321	30.463796
443.361830	22188.526026	30.468813
443.868417	22221.053461	30.473831
444.397796	22255.950267	30.478848
444.824442	22298.417024	30.483866
445.661788	22328.871625	30.488884
445.701487	22361.741497	30.493901
446.432538	22391.423821	30.498919
446.489465	22421.676607	30.503936
446.746143	22462.076316	30.508954
447.639133	22499.297599	30.513972
447.810815	22541.794543	30.518989
448.307782	22577.895762	30.524007
448.916286	22614.505262	30.529024
449.187675	22649.555951	30.534042
449.547130	22689.844584	30.539060
449.914681	22733.522182	30.544077
450.587653	22764.004768	30.549095
451.245365	22789.494482	30.554112
451.532300	22831.990425	30.559130
452.058117	22856.508650	30.564148
452.196457	22898.568907	30.569165
452.927260	22924.199684	30.574183
453.526354	22960.395198	30.579200
453.455691	22986.984975	30.584218
453.751556	23014.039236	30.589236
454.352408	23066.908493	30.594253
454.899658	23086.924688	30.599271
455.360409	23131.600239	30.604288
455.689541	23163.375139	30.609306
456.448085	23203.553218	30.614324
456.651001	23239.004366	30.619341
457.106977	23281.336267	30.624359
457.455093	23326.212311	30.629376
458.190997	23363.321143	30.634394
458.686821	23395.611345	30.639412
458.969654	23429.805489	30.644429
459.839383	23470.740061	30.649447
460.395520	23501.765264	30.654464
460.451775	23543.749236	30.659482
461.075660	23568.949260	30.664500
461.521393	23612.761253	30.669517
462.188817	23645.012494	30.674535
462.560751	23679.061508	30.679552
462.759675	23718.975448	30.684570
463.550379	23763.681634	30.689588
463.872059	23803.578612	30.694605
464.128092	23841.805523	30.699623
464.414678	23881.512949	30.704640
464.998286	23918.231879	30.709658
465.501905	23960.152305	30.714676
465.757939	24011.004703	30.719693
466.529174	24050.881482	30.724711
467.307132	24093.838637	30.729728
467.342477	24131.241691	30.734746
468.266979	24158.600601	30.739764
468.421217	24211.268189	30.744781
468.960792	24250.496207	30.749799
469.346175	24281.767133	30.754816
469.676159	24335.304901	30.759834
470.600761	24372.438323	30.764852
470.794821	24415.584376	30.769869
470.996536	24457.038725	30.774887
471.704972	24491.602972	30.779904
471.706612	24539.811822	30.784922
472.675600	24577.777315	30.789940
473.252400	24626.455802	30.794957
473.584664	24666.964925	30.799975
474.360935	24696.711604	30.804992
474.216250	24745.967158	30.810010
475.152841	24783.670375	30.815028
475.602995	24834.108298	30.820045
476.158782	24869.102289	30.825063
476.690963	24917.495658	30.830080
476.934438	24960.243797	30.835098
477.990832	24985.503661	30.840116
478.291537	25023.990764	30.845133
478.375797	25065.421862	30.850151
478.941811	25101.871837	30.855168
479.324155	25146.414233	30.860186
480.082933	25181.457279	30.865204
480.443792	25219.089557	30.870221
481.094465	25263.739254	30.875239
481.770178	25299.856082	30.880256
482.017069	25337.280379	30.885274
482.528276	25367.788083	30.890292
482.979877	25412.871689	30.895309
483.371481	25443.717892	30.900327
483.590814	25467.133003	30.905344
483.812449	25504.479833	30.910362
484.543386	25531.882439	30.915380
484.352688	25583.251853	30.920397
485.148069	25616.403515	30.925415
485.946068	25662.531276	30.930432
486.146469	25707.127311	30.935450
486.255525	25744.073778	30.940468
486.798319	25798.013022	30.945485
487.327605	25848.611157	30.950503
487.963077	25891.088562	30.955520
488.328041	25947.937546	30.960538
488.983790	25999.168132	30.965556
489.637384	26039.766106	30.970573
489.887438	26101.340813	30.975591
490.188809	26130.386299	30.980608
490.833751	26192.571010	30.985626
491.377480	26243.678915	30.990644
491.870328	26283.354609	30.995661
492.490572	26342.222431	31.000679
493.194166	26380.273685	31.005696
493.797855	26436.586387	31.010714
494.604450	26472.633552	31.015732
494.963246	26513.603169	31.020749
495.673709	26553.088910	31.025767
496.119143	26588.877487	31.030784
496.601496	26630.893122	31.035802
497.079822	26672.780195	31.040820
497.541912	26707.468528	31.045837
497.687745	26758.221106	31.050855
498.482206	26801.336874	31.055872
498.648609	26857.679145	31.060890
499.360410	26892.925874	31.065908
499.997981	26951.635183	31.070925
500.418539	26991.412790	31.075943
501.066704	27038.231465	31.080960
500.966300	27085.249840	31.085978
501.306906	27132.387792	31.090996
502.172355	27192.145353	31.096013
502.327083	27237.418492	31.101031
503.220558	27284.925934	31.106048
503.612423	27340.065293	31.111066
504.360732	27379.000925	31.116084
504.697122	27434.137144	31.121101
504.970650	27484.637280	31.126119
506.012224	27529.275478	31.131136
506.335875	27575.751827	31.136154
506.693188	27626.361540	31.141172
507.401654	27672.629362	31.146189
508.115267	27724.846028	31.151207
508.799422	27760.493424	31.156224
508.690089	27808.568870	31.161242
509.449904	27846.888500	31.166260
510.315761	27891.553553	31.171277
510.963961	27945.573536	31.176295
511.606555	27977.404834	31.181312
511.731464	28030.158325	31.186330
512.070750	28073.261093	31.191348
512.399612	28122.249152	31.196365
512.910805	28170.349105	31.201383
513.829995	28211.267861	31.206400
514.047499	28269.325558	31.211418
514.400492	28311.805172	31.216436
515.178165	28350.438430	31.221453
515.155508	28410.224105	31.226471
516.233852	28441.763320	31.231488
516.475622	28500.619071	31.236506
516.826184	28544.393098	31.241524
517.350285	28584.785016	31.246541
518.112900	28633.948812	31.251559
518.691725	28675.660041	31.256576
518.693852	28731.615978	31.261594
519.252880	28773.437979	31.266612
519.643877	28813.335065	31.271629
519.846168	28876.716284	31.276647
520.485615	28920.563335	31.281664
521.390842	28983.345941	31.286682
521.822198	29037.859486	31.291700
522.326616	29087.001030	31.296717
522.751431	29141.361392	31.301735
523.723714	29191.747699	31.306752
523.828389	29251.041949	31.311770
524.271127	29303.503770	31.316788
524.684137	29359.775469	31.321805
525.072428	29424.730580	31.326823
525.730029	29468.916734	31.331840
526.223453	29540.010114	31.336858
526.887660	29584.744424	31.341876
527.691251	29648.773507	31.346893
528.024316	29709.028477	31.351911
528.463474	29750.790621	31.356928
529.106903	29826.381405	31.361946
529.395923	29883.047586	31.366964
530.297488	29939.309716	31.371981
530.956548	29993.624498	31.376999
531.746264	30056.013606	31.382016
532.226103	30106.323123	31.387034
532.546871	30149.901017	31.392052
533.188784	30197.284501	31.397069
533.777606	30258.779986	31.402087
534.202740	30310.146617	31.407104
534.489142	30362.643784	31.412122
534.761870	30421.794286	31.417140
535.911272	30480.620089	31.422157
536.389353	30540.645679	31.427175
537.250719	30592.499408	31.432192
537.780152	30650.333536	31.437210
538.240708	30699.357495	31.442228
538.657990	30742.819925	31.447245
539.135068	30792.551316	31.452263
540.151144	30845.632788	31.457280
540.527512	30898.504751	31.462298
541.084473	30945.815963	31.467316
541.673577	30989.667056	31.472333
542.138179	31052.239699	31.477351
542.708764	31095.541960	31.482368
543.407930	31155.668738	31.487386
544.011994	31201.003988	31.492404
544.553699	31251.947053	31.497421
544.295035	31298.308766	31.502439
545.176580	31358.178880	31.507456
545.836381	31416.423065	31.512474
546.166409	31463.599675	31.517492
546.721680	31509.025826	31.522509
546.979457	31569.924365	31.527527
547.858154	31622.302036	31.532544
548.228565	31690.783469	31.537562
548.886488	31753.651607	31.542580
549.253815	31799.955229	31.547597
549.943431	31867.242300	31.552615
550.548440	31915.819764	31.557632
550.968967	31986.707893	31.562650
551.209422	32040.773245	31.567668
552.265073	32094.116978	31.572685
552.683069	32154.460911	31.577703
552.933377	32197.437062	31.582720
553.265839	32250.061587	31.587738
553.794880	32311.451054	31.592756
554.394118	32371.033678	31.597773
554.584378	32436.256683	31.602791
555.649746	32497.292995	31.607808
556.071179	32549.566053	31.612826
556.221671	32621.173509	31.617844
557.337103	32673.515121	31.622861
557.722084	32733.866486	31.627879
558.624301	32795.621874	31.632896
558.922651	32851.671239	31.637914
559.602825	32909.352123	31.642932
560.158171	32966.728827	31.647949
560.230867	33039.994874	31.652967
561.007142	33094.678463	31.657984
561.997427	33157.796362	31.663002
561.935389	33228.655687	31.668020
562.985783	33288.475986	31.673037
563.406120	33349.315859	31.678055
563.868072	33420.483698	31.683072
564.517759	33478.187247	31.688090
564.940314	33546.064475	31.693108
565.885399	33600.645953	31.698125
566.004043	33673.045503	31.703143
566.397409	33743.907257	31.708160
567.285530	33801.357815	31.713178
567.754287	33880.939420	31.718196
568.908466	33945.042814	31.723213
569.483960	34010.794800	31.728231
569.954795	34074.607790	31.733248
570.653678	34123.680670	31.738266
570.920607	34198.437240	31.743284
571.959154	34251.039209	31.748301
572.428410	34311.820617	31.753319
573.218328	34373.265540	31.758336
573.693273	34428.631077	31.763354
574.246329	34498.030353	31.768372
575.030537	34562.064631	31.773389
575.233636	34619.391317	31.778407
575.872986	34672.685429	31.783424
576.855224	34734.229160	31.788442
577.303782	34804.489523	31.793460
577.668734	34842.984377	31.798477
578.172171	34904.926656	31.803495
578.841762	34973.494274	31.808512
579.534527	35038.293329	31.813530
579.788305	35106.620974	31.818548
580.082125	35162.564715	31.823565
580.468199	35229.024721	31.828583
581.286748	35306.149953	31.833600
582.298835	35364.250923	31.838618
582.395270	35434.029181	31.843636
583.450913	35497.617923	31.848653
584.002445	35564.424197	31.853671
584.488482	35624.620257	31.858688
585.259953	35679.571335	31.863706
585.875871	35752.442983	31.868724
586.509897	35815.629202	31.873741
586.933137	35873.450518	31.878759
587.480574	35930.651819	31.883776
588.074147	35987.186050	31.888794
588.674125	36062.640097	31.893812
589.222685	36115.429597	31.898829
589.596293	36183.545819	31.903847
590.497224	36252.168402	31.908864
591.276494	36309.259956	31.913882
591.272759	36378.121066	31.918900
592.216860	36422.283425	31.923917
592.676730	36484.112094	31.928935
593.486908	36544.917230	31.933952
593.834372	36600.373661	31.938970
594.341298	36659.670205	31.943988
595.127559	36712.753522	31.949005
595.457189	36784.044945	31.954023
595.811481	36843.714528	31.959040
596.765052	36908.748588	31.964058
597.024994	36975.299012	31.969076
597.986040	37038.612151	31.974093
598.495098	37102.694670	31.979111
599.034843	37158.180964	31.984128
599.539801	37216.166645	31.989146
600.110544	37293.290863	31.994164
600.958830	37348.865569	31.999181
601.498549	37426.472088	32.004199
601.823641	37488.190758	32.009216
602.843330	37554.163094	32.014234
602.947101	37628.045521	32.019252
604.044058	37687.295151	32.024269
604.499855	37765.743969	32.029287
605.156251	37827.775118	32.034304
605.665800	37891.629922	32.039322
605.932927	37962.671171	32.044340
606.975430	38028.499416	32.049357
607.545281	38098.064406	32.054375
607.865323	38174.810875	32.059392
608.753912	38244.064860	32.064410
609.241615	38317.050096	32.069428
609.890091	38388.875848	32.074445
610.773993	38461.250040	32.079463
611.284695	38528.664257	32.084480
611.938337	38585.477576	32.089498
612.807864	38660.781032	32.094516
613.214412	38723.377392	32.099533
613.777007	38805.089501	32.104551
614.538151	38869.193348	32.109568
615.485684	38936.833517	32.114586
615.775392	39006.953370	32.119604
616.246812	39076.819309	32.124621
616.922760	39143.207809	32.129639
617.504007	39213.153953	32.134656
618.356890	39274.062161	32.139674
618.951284	39347.125399	32.144692
619.718094	39417.556158	32.149709
620.112621	39480.163407	32.154727
620.482738	39546.651317	32.159744
621.235314	39616.750587	32.164762
621.813945	39694.843280	32.169780
622.623683	39768.541792	32.174797
623.345017	39824.419681	32.179815
623.545308	39903.702808	32.184832
624.477122	39962.936642	32.189850
624.979060	40044.818991	32.194868
625.823953	40105.421918	32.199885
626.186092	40184.979375	32.204903
626.840522	40248.373322	32.209920
627.948849	40311.919686	32.214938
628.164666	40399.514277	32.219956
628.902297	40461.607207	32.224973
629.157018	40529.923474	32.229991
629.673306	40607.361101	32.235008
630.524450	40679.481136	32.240026
631.335479	40759.130964	32.245044
632.031558	40818.150843	32.250061
632.963950	40897.058257	32.255079
633.284084	40964.156210	32.260096
634.275257	41010.152918	32.265114
634.707372	41081.283118	32.270132
635.098302	41137.244909	32.275149
635.817518	41187.943564	32.280167
636.619863	41253.763145	32.285184
637.337405	41311.647697	32.290202
637.416545	41378.594447	32.295220
637.875365	41443.183480	32.300237
638.701392	41512.324394	32.305255
639.155345	41595.970551	32.310272
639.656920	41656.726928	32.315290
640.439483	41745.992608	32.320308
640.938640	41813.297643	32.325325
641.788229	41880.352366	32.330343
642.407134	41954.166951	32.335360
642.956061	42021.568692	32.340378
643.362876	42106.118407	32.345396
644.289019	42192.360059	32.350413
645.048838	42263.497409	32.355431
645.464959	42348.352930	32.360448
646.326353	42414.353137	32.365466
646.557842	42502.403393	32.370484
647.275051	42571.578886	32.375501
647.943927	42653.369384	32.380519
648.261745	42733.466058	32.385536
649.344211	42822.191608	32.390554
650.271420	42906.071617	32.395572
650.590788	42987.826687	32.400589
651.314988	43064.195117	32.405607
651.800473	43148.752336	32.410624
652.552891	43212.926383	32.415642
653.414291	43303.771463	32.420660
653.996328	43389.210478	32.425677
654.879585	43478.783543	32.430695
655.299418	43563.337712	32.435712
656.261701	43644.357819	32.440730
656.552562	43725.337799	32.445748
657.328249	43816.196392	32.450765
658.104789	43882.253721	32.455783
658.674121	43972.414688	32.460800
659.613183	44043.702833	32.465818
660.240996	44135.484153	32.470836
660.808032	44211.700136	32.475853
662.064067	44282.965172	32.480871
662.611573	44363.507606	32.485888
663.377459	44431.671532	32.490906
663.951983	44505.677210	32.495924
664.493313	44585.511174	32.500941
665.100694	44656.291320	32.505959
665.592309	44739.629572	32.510976
666.451552	44811.300117	32.515994
667.247944	44888.781826	32.521012
667.509132	44962.124363	32.526029
668.331490	45041.064374	32.531047
669.093260	45126.386835	32.536064
669.652873	45197.262174	32.541082
669.974360	45279.074239	32.546100
670.968857	45360.219573	32.551117
671.741348	45438.114835	32.556135
672.317501	45522.500387	32.561152
673.026297	45594.050388	32.566170
673.598668	45674.414324	32.571188
674.330327	45757.404749	32.576205
675.121074	45833.583972	32.581223
675.674064	45911.650124	32.586240
676.396256	45997.481997	32.591258
677.027784	46068.705537	32.596276
678.050908	46145.100197	32.601293
678.428550	46217.850464	32.606311
679.179444	46293.649722	32.611328
680.019923	46357.548366	32.616346
680.874141	46423.036508	32.621364
681.051467	46493.092590	32.626381
682.035141	46557.947158	32.631399
682.710698	46628.410788	32.636416
683.284965	46696.838806	32.641434
683.888735	46765.846402	32.646452
684.624985	46842.916598	32.651469
685.028705	46912.017819	32.656487
685.612889	46985.273708	32.661504
686.593165	47083.958520	32.666522
687.260458	47151.933832	32.671540
687.669598	47228.674432	32.676557
688.451441	47311.088602	32.681575
689.038197	47397.107109	32.686592
689.656587	47470.716062	32.691610
690.376571	47562.075593	32.696628
690.805407	47639.064071	32.701645
691.731404	47717.963354	32.706663
692.253172	47813.509729	32.711680
692.725445	47899.413641	32.716698
693.724429	47989.342662	32.721716
693.992793	48081.647867	32.726733
695.194842	48165.834244	32.731751
695.577038	48263.433480	32.736768
696.008351	48354.932983	32.741786
697.020856	48446.008330	32.746804
697.596168	48545.418275	32.751821
698.692274	48629.684226	32.756839
699.308128	48726.877658	32.761856
699.567987	48819.127815	32.766874
700.541563	48907.779949	32.771892
701.572287	49015.938012	32.776909
702.231827	49096.241956	32.781927
703.145471	49191.082926	32.786944
703.952011	49275.560690	32.791962
704.616905	49359.768531	32.796980
704.982798	49459.066247	32.801997
706.150093	49538.596367	32.807015
706.810885	49633.835085	32.812032
707.545545	49711.242415	32.817050
708.372725	49809.767628	32.822068
709.169796	49895.194040	32.827085
710.038306	49975.274421	32.832103
710.475269	50055.881337	32.837120
711.244233	50140.545983	32.842138
711.953407	50222.198233	32.847156
712.402622	50314.332629	32.852173
713.640972	50399.261880	32.857191
714.144053	50482.436975	32.862208
714.784284	50570.637070	32.867226
715.648066	50654.410211	32.872244
716.079260	50741.862346	32.877261
717.199595	50813.300636	32.882279
717.708822	50911.024928	32.887296
718.419776	50998.027642	32.892314
719.268976	51080.402621	32.897332
719.836753	51175.680113	32.902349
720.319180	51256.417168	32.907367
721.117480	51338.795346	32.912384
721.936082	51433.148186	32.917402
722.822178	51502.056606	32.922420
723.058534	51593.821662	32.927437
724.134059	51678.979299	32.932455
724.519639	51766.930035	32.937472
725.072050	51859.275805	32.942490
726.179710	51930.973007	32.947508
726.631558	52017.265044	32.952525
727.326192	52100.573320	32.957543
727.714436	52188.342307	32.962560
728.664010	52272.506244	32.967578
729.516685	52362.024977	32.972596
729.881988	52448.554354	32.977613
730.758327	52533.754993	32.982631
731.775577	52637.355185	32.987648
732.548037	52711.606209	32.992666
733.275678	52800.958104	32.997684
733.990983	52890.122914	33.002701
734.739379	52961.163101	33.007719
735.496262	53061.118992	33.012736
736.111146	53136.490685	33.017754
736.963508	53230.707640	33.022772
737.557363	53334.590048	33.027789
738.380088	53411.147783	33.032807
739.093828	53505.761749	33.037824
739.533847	53594.514083	33.042842
740.470362	53691.372905	33.047860
741.254922	53786.728360	33.052877
741.722498	53879.830594	33.057895
742.713020	53975.544619	33.062912
743.371483	54074.239360	33.067930
744.445642	54166.484429	33.072948
744.897923	54263.571486	33.077965
745.476015	54358.736406	33.082983
746.324930	54453.294659	33.088000
746.960388	54551.338488	33.093018
748.256529	54652.837082	33.098036
748.893546	54756.694580	33.103053
749.439401	54849.990633	33.108071
750.179331	54941.814413	33.113088
751.101791	55035.579798	33.118106
751.885164	55125.937674	33.123124
752.844472	55230.951189	33.128141
753.372355	55327.171639	33.133159
754.651800	55420.917712	33.138176
755.197091	55517.660652	33.143194
755.911269	55606.610469	33.148212
756.654603	55701.008908	33.153229
757.446670	55793.763181	33.158247
758.461658	55881.533419	33.163264
758.638729	55993.435123	33.168282
759.669369	56069.027272	33.173300
760.475738	56177.110448	33.178317
761.333380	56262.576736	33.183335
761.936288	56358.334808	33.188352
762.534638	56458.763798	33.193370
763.656997	56546.209581	33.198388
764.264040	56657.968067	33.203405
765.033059	56748.247229	33.208423
765.535911	56847.404887	33.213440
766.324965	56948.316641	33.218458
767.423678	57036.097077	33.223476
767.889487	57142.731543	33.228493
768.784424	57236.423390	33.233511
769.678354	57336.289727	33.238528
769.836473	57439.956079	33.243546
771.026723	57530.908453	33.248564
771.594317	57635.253761	33.253581
772.292294	57727.899882	33.258599
773.143657	57828.742574	33.263616
773.890207	57939.208621	33.268634
774.998507	58041.039947	33.273652
775.529881	58142.657560	33.278669
776.469041	58245.130887	33.283687
777.041431	58331.676958	33.288704
777.642938	58427.255568	33.293722
778.952694	58502.753878	33.298740
779.505246	58606.405240	33.303757
780.361079	58693.013415	33.308775
780.639258	58790.726395	33.313792
781.765171	58870.427485	33.318810
782.611514	58968.552927	33.323828
783.175315	59066.706619	33.328845
783.786932	59161.092598	33.333863
785.034476	59256.170132	33.338880
785.272271	59361.615385	33.343898
785.836941	59454.146137	33.348916
786.555296	59558.602864	33.353933
786.994517	59675.360698	33.358951
788.306015	59776.035903	33.363968
789.592489	59885.987224	33.368986
790.296315	59983.667159	33.374004
790.911779	60089.559332	33.379021
791.637930	60197.930199	33.384039
792.682807	60295.510982	33.389056
793.137993	60407.802039	33.394074
794.237609	60511.315783	33.399092
795.213869	60617.789374	33.404109
795.766112	60715.118680	33.409127
796.217555	60827.172496	33.414144
796.910003	60938.137888	33.419162
798.145460	61043.363644	33.424180
798.602138	61160.626423	33.429197
799.457545	61273.020378	33.434215
800.884097	61371.965293	33.439232
800.875357	61496.682987	33.444250
801.967379	61603.142573	33.449268
802.748796	61715.437427	33.454285
803.706618	61842.727855	33.459303
804.903296	61947.553841	33.464320
805.441886	62063.544110	33.469338
806.459493	62169.443764	33.474356
807.205112	62278.214333	33.479373
807.797736	62395.126690	33.484391
809.100116	62492.112826	33.489408
809.437389	62611.660189	33.494426
810.501628	62723.641983	33.499444
810.987897	62831.996951	33.504461
811.604010	62944.566061	33.509479
813.085469	63055.918090	33.514496
813.522516	63170.174151	33.519514
814.711587	63282.479672	33.524532
815.540320	63384.832772	33.529549
816.350057	63497.720536	33.534567
816.854320	63607.182794	33.539584
817.652657	63727.747603	33.544602
818.789899	63828.642245	33.549620
819.209680	63938.663855	33.554637
820.308398	64063.359298	33.559655
821.069033	64162.775457	33.564672
821.821880	64286.006000	33.569690
822.763713	64391.752595	33.574708
823.358932	64520.042442	33.579725
823.749944	64633.644112	33.584743
825.358236	64738.270805	33.589760
826.165121	64859.725788	33.594778
826.914166	64963.617033	33.599796
827.804623	65083.681395	33.604813
828.293490	65192.193665	33.609831
829.138793	65303.182544	33.614848
829.711504	65424.622652	33.619866
830.884527	65540.457927	33.624884
831.825283	65644.080627	33.629901
832.423185	65735.053688	33.634919
833.639347	65847.532968	33.639936
834.237876	65952.781618	33.644954
835.269200	66050.682693	33.649972
835.978334	66160.187705	33.654989
836.362228	66259.966982	33.660007
837.412619	66368.556853	33.665024
838.042575	66476.496109	33.670042
838.903446	66583.518961	33.675060
839.586783	66703.310767	33.680077
840.324146	66826.287003	33.685095
841.352153	66946.092730	33.690112
841.971750	67063.829776	33.695130
842.938419	67175.377493	33.700148
843.758053	67298.640026	33.705165
844.358258	67423.513829	33.710183
845.572614	67544.158294	33.715200
846.295128	67665.656127	33.720218
847.675590	67772.472637	33.725236
848.169207	67892.789402	33.730253
848.704146	68010.077862	33.735271
850.101772	68133.521539	33.740288
850.839330	68258.364909	33.745306
851.724894	68375.331853	33.750324
852.779189	68502.672288	33.755341
853.045699	68612.693173	33.760359
854.306425	68733.975342	33.765376
855.288923	68855.614033	33.770394
856.038654	68975.666960	33.775412
857.014867	69093.552317	33.780429
857.551640	69219.484127	33.785447
858.932672	69338.562137	33.790464
859.944281	69457.942182	33.795482
860.689389	69571.581457	33.800500
861.808845	69688.700305	33.805517
862.688189	69815.830931	33.810535
863.600795	69931.012530	33.815552
864.285477	70044.778130	33.820570
865.427398	70160.574319	33.825588
866.592626	70267.495872	33.830605
867.184558	70389.353331	33.835623
868.020527	70503.127960	33.840640
868.829990	70617.666369	33.845658
869.646657	70735.713632	33.850676
870.519185	70840.726226	33.855693
871.053898	70959.447359	33.860711
872.244433	71080.627989	33.865728
873.018313	71205.387720	33.870746
873.653694	71315.753546	33.875764
874.635969	71433.277693	33.880781
875.165681	71554.152922	33.885799
876.419705	71681.061888	33.890816
877.099814	71808.736818	33.895834
877.977313	71935.918230	33.900852
879.144055	72057.671091	33.905869
879.887464	72188.449051	33.910887
881.023282	72294.127111	33.915904
881.709004	72415.733881	33.920922
882.529884	72549.290001	33.925940
883.854723	72669.913486	33.930957
884.060440	72787.244572	33.935975
885.413598	72898.941616	33.940992
886.164255	73027.756689	33.946010
886.959097	73148.742414	33.951028
887.743851	73269.800044	33.956045
888.702668	73400.258768	33.961063
889.656684	73511.569633	33.966080
890.337285	73632.507371	33.971098
891.216335	73741.757486	33.976116
892.272671	73855.854799	33.981133
892.923702	73969.709849	33.986151
893.850399	74083.045580	33.991168
894.808966	74200.006785	33.996186
895.532326	74317.228865	34.001204
896.509576	74430.248141	34.006221
897.020865	74552.407946	34.011239
898.341339	74670.064415	34.016256
898.995176	74802.137751	34.021274
899.907959	74920.912852	34.026292
901.165634	75047.726993	34.031309
901.506709	75177.413024	34.036327
902.774986	75292.349233	34.041344
903.371221	75427.781577	34.046362
904.120099	75547.257578	34.051380
905.298616	75679.192482	34.056397
905.838330	75823.858076	34.061415
906.850491	75947.207741	34.066432
908.052776	76084.175687	34.071450
908.576224	76209.125598	34.076468
909.894031	76338.024426	34.081485
910.784199	76484.597110	34.086503
911.772772	76616.018740	34.091520
912.801311	76742.089877	34.096538
913.642029	76876.775924	34.101556
914.520822	77013.221199	34.106573
915.397469	77145.556313	34.111591
916.520637	77271.924738	34.116608
917.670668	77412.559161	34.121626
918.254710	77534.837253	34.126644
919.273677	77668.670002	34.131661
919.899005	77813.321737	34.136679
920.955954	77947.624277	34.141696
921.611073	78081.437437	34.146714
922.387623	78227.705128	34.151732
923.413788	78371.503500	34.156749
924.429691	78508.270487	34.161767
925.352755	78647.596544	34.166784
926.213737	78789.343795	34.171802
926.880871	78932.869878	34.176820
928.511141	79075.364658	34.181837
929.107325	79222.895842	34.186855
930.111128	79364.755940	34.191872
931.368941	79509.048322	34.196890
931.933765	79653.000764	34.201908
933.206008	79779.618031	34.206925
933.946031	79923.960736	34.211943
934.770889	80061.711313	34.216960
936.039911	80200.616526	34.221978
936.759187	80353.341047	34.226996
938.234552	80484.730153	34.232013
938.939362	80630.867143	34.237031
940.020574	80759.058730	34.242048
940.653252	80905.373894	34.247066
941.847769	81046.833420	34.252084
942.830596	81180.705652	34.257101
943.642221	81315.347161	34.262119
944.639008	81453.084070	34.267136
945.528951	81591.187432	34.272154
946.411437	81739.794758	34.277172
947.342416	81862.690532	34.282189
948.238781	82008.716108	34.287207
949.578589	82151.436414	34.292224
950.365557	82275.098425	34.297242
951.050499	82422.262425	34.302260
952.183500	82558.015880	34.307277
952.458947	82697.119585	34.312295
953.675781	82834.075537	34.317312
954.898617	82958.586531	34.322330
955.289276	83100.862323	34.327348
956.807652	83220.080928	34.332365
957.440216	83370.049794	34.337383
958.153235	83498.924994	34.342400
958.928831	83632.194132	34.347418
959.938581	83786.987750	34.352436
961.189774	83919.895187	34.357453
961.862411	84074.885672	34.362471
962.594203	84212.853769	34.367488
963.576813	84363.290012	34.372506
964.757297	84510.423346	34.377524
965.685307	84651.936478	34.382541
966.360301	84810.120411	34.387559
967.606218	84962.642964	34.392576
968.718562	85118.826841	34.397594
969.523931	85275.347259	34.402612
970.581796	85431.877594	34.407629
971.573651	85579.447504	34.412647
972.210474	85743.901974	34.417664
973.238861	85894.637929	34.422682
974.060164	86060.392908	34.427700
975.083461	86203.475268	34.432717
976.124349	86373.929246	34.437735
977.304021	86539.754906	34.442752
978.033116	86700.840789	34.447770
978.933892	86868.841026	34.452788
980.250944	87030.509021	34.457805
981.229000	87196.442253	34.462823
982.310604	87355.120328	34.467840
983.406620	87514.334967	34.472858
984.087420	87676.435323	34.477876
985.254745	87838.063996	34.482893
986.357187	87999.596923	34.487911
987.480142	88158.994959	34.492928
988.494653	88318.095587	34.497946
989.622025	88482.766483	34.502964
991.139344	88630.793856	34.507981
992.200351	88789.453296	34.512999
993.023252	88943.254987	34.518016
994.389234	89084.595780	34.523034
994.476526	89242.995239	34.528052
995.819313	89401.226119	34.533069
997.359982	89557.330574	34.538087
998.232118	89713.844035	34.543104
999.240271	89860.007689	34.548122
1000.231312	90010.788670	34.553140
1001.213549	90169.710785	34.558157
1002.000914	90317.318707	34.563175
1003.268618	90476.398169	34.568192
1004.319224	90625.540328	34.573210
1004.865372	90782.532356	34.578228
1005.807668	90941.662368	34.583245
1007.045780	91097.934457	34.588263
1007.601519	91257.244386	34.593280
1008.954173	91411.524914	34.598298
1009.992578	91577.130490	34.603316
1010.895036	91729.500150	34.608333
1012.032260	91892.490270	34.613351
1012.765439	92060.649638	34.618368
1013.994441	92208.689765	34.623386
1014.617395	92376.179652	34.628404
1016.138382	92527.686200	34.633421
1017.182697	92691.792015	34.638439
1018.116453	92855.885567	34.643456
1019.456252	92998.443556	34.648474
1020.189452	93149.153793	34.653492
1021.274981	93288.293282	34.658509
1022.075420	93431.651885	34.663527
1022.862469	93584.723158	34.668544
1024.059362	93724.061915	34.673562
1024.609981	93885.383706	34.678580
1025.656595	94040.484710	34.683597
1026.845806	94191.898181	34.688615
1027.503332	94355.756274	34.693632
1028.927716	94510.411659	34.698650
1029.646786	94673.786951	34.703668
1030.447611	94826.091420	34.708685
1032.107058	94987.711831	34.713703
1032.936937	95157.984327	34.718720
1033.993025	95320.308024	34.723738
1035.219431	95474.710995	34.728756
1035.924538	95639.329334	34.733773
1037.134097	95799.801383	34.738791
1038.045653	95974.718657	34.743808
1038.971335	96136.499528	34.748826
1040.129464	96315.607042	34.753844
1041.257667	96480.983929	34.758861
1042.161494	96640.233211	34.763879
1043.186951	96829.425335	34.768896
1044.451435	96986.059692	34.773914
1045.434673	97162.758628	34.778932
1046.634042	97329.889244	34.783949
1047.586983	97503.367001	34.788967
1048.402973	97685.522598	34.793984
1049.674267	97850.346757	34.799002
1050.935573	98035.210431	34.804020
1051.894584	98204.747966	34.809037
1053.248275	98371.214242	34.814055
1054.013019	98549.763322	34.819072
1055.093945	98715.814812	34.824090
1055.971398	98884.287801	34.829108
1057.219209	99066.109725	34.834125
1058.686796	99241.527587	34.839143
1059.335464	99415.587921	34.844160
1060.503117	99581.472458	34.849178
1061.576754	99751.425568	34.854196
1062.708843	99935.298812	34.859213
1063.909207	100105.866452	34.864231
1064.885721	100284.937188	34.869248
1066.368873	100447.710845	34.874266
1067.079226	100621.218372	34.879284
1068.175718	100794.302339	34.884301
1069.528715	100970.384170	34.889319
1070.434852	101139.874007	34.894336
1071.745748	101306.885720	34.899354
1072.600936	101483.667530	34.904372
1073.815216	101646.182989	34.909389
1074.925673	101819.353853	34.914407
1075.796218	101982.681731	34.919424
1077.054461	102154.323457	34.924442
1078.442093	102340.197819	34.929460
1079.252627	102512.688420	34.934477
1080.631847	102673.087220	34.939495
1081.345198	102849.300278	34.944512
1082.771486	103016.360936	34.949530
1083.451833	103185.097337	34.954548
1084.236622	103359.510076	34.959565
1085.525270	103525.691273	34.964583
1086.534315	103706.939578	34.969600
1087.670802	103885.888484	34.974618
1089.047294	104053.666887	34.979636
1090.068119	104230.256353	34.984653
1091.079255	104395.070523	34.989671
1091.700242	104553.161960	34.994688
1092.974531	104731.093337	34.999706
1093.983586	104893.479339	35.004724
1095.080532	105068.668716	35.009741
1096.228362	105230.932533	35.014759
1097.351565	105395.075851	35.019776
1098.515586	105557.376991	35.024794
1099.473001	105731.656608	35.029812
1100.607310	105896.814421	35.034829
1101.868510	106070.792737	35.039847
1102.700568	106240.790185	35.044864
1103.641569	106413.835775	35.049882
1104.890361	106580.828085	35.054900
1105.490514	106756.946680	35.059917
1107.012847	106941.007434	35.064935
1107.876662	107119.959973	35.069952
1108.786049	107313.446735	35.074970
1110.018357	107493.290797	35.079988
1111.006902	107680.674738	35.085005
1112.261551	107866.078055	35.090023
1113.116680	108053.828642	35.095040
1114.400994	108238.748302	35.100058
1115.513541	108430.398218	35.105076
1116.518707	108625.461899	35.110093
1117.975385	108819.337673	35.115111
1118.891484	109009.491500	35.120128
1119.902785	109203.798328	35.125146
1121.088899	109405.006482	35.130164
1122.195054	109606.419351	35.135181
1123.659985	109794.372540	35.140199
1124.474283	110006.071682	35.145216
1125.674335	110197.288923	35.150234
1126.554629	110395.324776	35.155252
1127.567449	110600.167952	35.160269
1129.135273	110793.456706	35.165287
1130.094804	111008.559850	35.170304
1131.250579	111200.754163	35.175322
1132.434734	111405.473680	35.180340
1133.418837	111612.178663	35.185357
1134.931089	111816.200922	35.190375
1135.960084	112027.512779	35.195392
1137.072406	112226.093519	35.200410
1138.338661	112433.961487	35.205428
1139.394941	112633.010468	35.210445
1140.924699	112830.576391	35.215463
1141.289930	113041.030218	35.220480
1142.866675	113249.182338	35.225498
1144.441145	113451.420041	35.230516
1145.113181	113651.261942	35.235533
1146.575492	113845.134207	35.240551
1147.207763	114071.628630	35.245568
1148.591115	114271.889466	35.250586
1149.755061	114475.596043	35.255604
1150.779540	114690.944982	35.260621
1152.304708	114900.220128	35.265639
1153.190724	115107.651370	35.270656
1154.632608	115315.828440	35.275674
1155.940945	115517.694236	35.280692
1156.777477	115726.405168	35.285709
1158.365427	115928.341691	35.290727
1159.119578	116135.612204	35.295744
1160.126099	116338.559999	35.300762
1161.068850	116546.917296	35.305780
1162.426578	116772.641870	35.310797
1163.979779	116976.454101	35.315815
1164.790241	117181.974379	35.320832
1165.683986	117392.740657	35.325850
1166.837129	117603.719014	35.330868
1167.810905	117805.897035	35.335885
1169.308641	117999.715783	35.340903
1170.267850	118208.183782	35.345920
1171.383536	118412.344603	35.350938
1172.566048	118618.611897	35.355956
1173.648098	118818.396929	35.360973
1174.661119	119027.140692	35.365991
1175.500152	119242.668575	35.371008
1176.707367	119453.284004	35.376026
1178.017713	119663.402386	35.381044
1179.062374	119889.570536	35.386061
1180.543452	120101.260476	35.391079
1181.533032	120324.171770	35.396096
1182.773596	120541.226832	35.401114
1184.447335	120766.309341	35.406132
1185.164164	120972.492828	35.411149
1186.718502	121190.996128	35.416167
1187.712034	121411.595980	35.421184
1188.931334	121635.835162	35.426202
1190.258233	121854.824499	35.431220
1191.247619	122083.350370	35.436237
1192.402231	122306.540812	35.441255
1193.910306	122534.186021	35.446272
1195.010359	122753.244816	35.451290
1196.345890	122970.796222	35.456308
1197.337956	123207.605734	35.461325
1198.602592	123427.719473	35.466343
1200.022108	123652.333588	35.471360
1200.844857	123878.163287	35.476378
1202.433559	124103.918757	35.481396
1203.657696	124338.113416	35.486413
1204.990472	124562.127642	35.491431
1206.052083	124796.466778	35.496448
1207.138115	125034.504455	35.501466
1208.302155	125256.688643	35.506484
1209.771480	125491.371307	35.511501
1210.880743	125717.610936	35.516519
1212.166917	125960.008018	35.521536
1213.409981	126188.687820	35.526554
1214.626707	126427.754054	35.531572
1216.155826	126661.104988	35.536589
1217.114617	126879.443798	35.541607
1218.617495	127115.033246	35.546624
1219.822713	127334.361194	35.551642
1221.059084	127559.959630	35.556660
1222.112714	127812.676415	35.561677
1223.934165	128027.572554	35.566695
1224.888306	128262.589652	35.571712
1226.258452	128490.720450	35.576730
1227.427453	128714.855392	35.581748
1228.708758	128946.718093	35.586765
1230.016559	129168.551756	35.591783
1231.093789	129398.055847	35.596800
1232.306074	129616.549413	35.601818
1233.892365	129850.650012	35.606836
1234.689184	130073.297041	35.611853
1236.208996	130301.644425	35.616871
1237.296558	130534.590279	35.621888
1238.729339	130763.601861	35.626906
1240.096067	130980.253949	35.631924
1241.045869	131206.280890	35.636941
1242.019707	131440.532492	35.641959
1243.469383	131669.142146	35.646976
1244.623719	131901.503835	35.651994
1246.180226	132138.871434	35.657012
1247.403242	132371.643508	35.662029
1248.827812	132594.140989	35.667047
1249.907590	132809.889440	35.672064
1250.631060	133027.815302	35.677082
1252.171090	133238.064736	35.682100
1253.208323	133451.441187	35.687117
1254.420541	133669.518770	35.692135
1255.567592	133892.261206	35.697152
1256.622348	134114.209058	35.702170
1258.056944	134336.907004	35.707188
1259.108491	134572.093927	35.712205
1260.605981	134788.166790	35.717223
1261.693909	135014.020020	35.722240
1263.035353	135252.130523	35.727258
1264.155512	135479.515655	35.732276
1265.565241	135711.342553	35.737293
1266.382528	135944.207189	35.742311
1267.671513	136184.069998	35.747328
1268.471695	136428.097782	35.752346
1270.044541	136669.438586	35.757364
1271.187091	136918.624243	35.762381
1272.674470	137167.387081	35.767399
1274.158664	137412.247229	35.772416
1275.318670	137667.711578	35.777434
1276.463394	137910.615529	35.782452
1277.653565	138160.550602	35.787469
1279.033397	138408.250005	35.792487
1281.033942	138662.378446	35.797504
1281.601284	138922.971241	35.802522
1283.121557	139169.511855	35.807540
1284.065906	139426.331117	35.812557
1285.738586	139675.487548	35.817575
1287.243922	139930.113060	35.822592
1288.319119	140192.913966	35.827610
1289.898905	140437.716760	35.832628
1290.999189	140685.263350	35.837645
1292.283749	140946.944932	35.842663
1293.759933	141203.524746	35.847680
1294.958894	141460.760935	35.852698
1296.311882	141705.141026	35.857716
1297.634865	141973.481209	35.862733
1298.595820	142239.905123	35.867751
1300.410292	142486.395479	35.872768
1301.092173	142755.063196	35.877786
1303.063678	143009.241180	35.882804
1304.388178	143278.111026	35.887821
1305.663700	143531.025585	35.892839
1307.235998	143794.367521	35.897856
1308.436555	144044.863367	35.902874
1310.187449	144294.952991	35.907892
1311.352777	144552.204696	35.912909
1312.789669	144799.712031	35.917927
1314.422938	145051.018464	35.922944
1315.652287	145308.658164	35.927962
1317.136083	145543.950446	35.932980
1318.284853	145801.239225	35.937997
1319.280916	146045.289777	35.943015
1320.972917	146292.689147	35.948032
1321.949630	146551.952058	35.953050
1323.437573	146785.958172	35.958068
1324.880267	147043.169153	35.963085
1326.035191	147301.431417	35.968103
1327.455030	147539.981235	35.973120
1328.443293	147793.379091	35.978138
1330.263068	148036.089327	35.983156
1331.624624	148292.891290	35.988173
1332.764936	148539.001960	35.993191
1334.510255	148789.947921	35.998208
1335.627006	149034.683349	36.003226
1337.120587	149278.191271	36.008244
1338.311347	149516.525385	36.013261
1339.605737	149746.295413	36.018279
1340.762866	149988.709411	36.023296
1341.970945	150214.666227	36.028314
1343.537225	150459.209871	36.033332
1344.569941	150695.231170	36.038349
1345.726630	150923.192051	36.043367
1346.999834	151161.066376	36.048384
1348.598881	151400.626021	36.053402
1349.895562	151646.743964	36.058420
1351.249315	151883.924583	36.063437
1352.051962	152143.534295	36.068455
1353.490533	152381.642607	36.073472
1354.483564	152642.479966	36.078490
1355.896374	152891.301148	36.083508
1357.453804	153156.310631	36.088525
1358.913438	153414.399712	36.093543
1360.223445	153668.988949	36.098560
1361.833482	153936.138766	36.103578
1363.033490	154198.855119	36.108596
1364.554070	154454.822704	36.113613
1365.390914	154716.968324	36.118631
1367.031736	154980.784093	36.123648
1368.383417	155254.848181	36.128666
1369.786425	155508.685623	36.133684
1370.943999	155796.434736	36.138701
1372.236950	156063.055243	36.143719
1373.803331	156329.873377	36.148736
1375.387652	156609.946642	36.153754
1376.896927	156878.021062	36.158772
1378.292583	157154.653486	36.163789
1379.470072	157425.551869	36.168807
1381.449086	157691.308726	36.173824
1382.559882	157972.268967	36.178842
1383.987623	158233.312542	36.183860
1385.563419	158508.034273	36.188877
1386.846648	158771.147644	36.193895
1388.599014	159043.649110	36.198912
1389.459579	159324.076478	36.203930
1390.997342	159591.593277	36.208948
1392.719581	159872.655867	36.213965
1393.788148	160138.071681	36.218983
1394.896348	160412.350616	36.224000
1396.509290	160697.420484	36.229018
1398.435548	160968.852948	36.234036
1399.697674	161249.252389	36.239053
1401.061781	161529.471926	36.244071
1402.872518	161798.404160	36.249088
1403.927711	162072.791573	36.254106
1405.460139	162343.765166	36.259124
1406.844488	162614.612718	36.264141
1408.013797	162896.383322	36.269159
1409.814443	163164.463173	36.274176
1410.854827	163439.914939	36.279194
1412.679813	163717.738289	36.284212
1414.092903	163997.217470	36.289229
1415.066370	164268.676296	36.294247
1416.710691	164531.296706	36.299264
1417.964925	164820.209190	36.304282
1419.264842	165107.707675	36.309300
1420.978767	165377.769592	36.314317
1422.120415	165654.056153	36.319335
1423.946091	165928.797646	36.324352
1425.102801	166214.969428	36.329370
1426.501203	166498.527374	36.334388
1428.071885	166767.238466	36.339405
1429.170952	167058.665598	36.344423
1430.913022	167333.074359	36.349440
1432.115578	167603.437424	36.354458
1433.605289	167870.392128	36.359476
1434.989811	168131.427390	36.364493
1436.182306	168397.837962	36.369511
1437.898535	168659.608189	36.374528
1439.105005	168929.394877	36.379546
1440.205180	169202.601442	36.384564
1441.933987	169480.629213	36.389581
1442.891768	169741.718886	36.394599
1444.787656	170020.826307	36.399616
1445.771387	170300.378010	36.404634
1446.946407	170579.379525	36.409652
1448.445369	170868.722036	36.414669
1449.659780	171157.199709	36.419687
1451.471077	171444.806459	36.424704
1452.645919	171746.618640	36.429722
1453.983195	172036.236220	36.434740
1456.122292	172335.139121	36.439757
1457.037215	172639.614135	36.444775
1458.716478	172937.873493	36.449792
1460.024279	173226.500705	36.454810
1461.722833	173541.080396	36.459828
1463.240746	173838.559863	36.464845
1464.485587	174138.522879	36.469863
1465.941276	174438.326015	36.474880
1467.480061	174743.599665	36.479898
1468.930495	175049.562444	36.484916
1470.691742	175352.836086	36.489933
1471.946193	175665.472433	36.494951
1473.781293	175972.341936	36.499968
1475.007597	176273.323743	36.504986
1476.627242	176587.669659	36.510004
1478.386549	176886.549221	36.515021
1479.771880	177199.757435	36.520039
1481.695047	177504.705467	36.525056
1483.192949	177800.549669	36.530074
1484.554881	178110.493026	36.535092
1485.961805	178418.692090	36.540109
1487.404331	178722.495805	36.545127
1489.147838	179024.690507	36.550144
1490.944961	179333.757131	36.555162
1492.351412	179649.604208	36.560180
1493.736220	179949.502916	36.565197
1495.247785	180253.342351	36.570215
1496.838319	180560.648170	36.575232
1498.391086	180865.385512	36.580250
1500.109146	181178.156942	36.585268
1501.193559	181467.744379	36.590285
1502.949084	181779.802414	36.595303
1504.602281	182084.238284	36.600320
1505.961950	182396.961901	36.605338
1507.832473	182693.470533	36.610356
1509.136586	182992.562171	36.615373
1510.525354	183305.628980	36.620391
1511.922247	183620.777894	36.625408
1513.683515	183932.174775	36.630426
1515.471777	184245.320615	36.635444
1516.803870	184537.587275	36.640461
1518.431020	184849.646189	36.645479
1520.111293	185146.377325	36.650496
1521.692023	185449.016200	36.655514
1522.794609	185758.450527	36.660532
1524.810203	186051.716562	36.665549
1526.040871	186358.594347	36.670567
1527.417360	186657.770081	36.675584
1529.263163	186965.412691	36.680602
1530.406578	187276.244902	36.685620
1531.995257	187562.671215	36.690637
1533.333515	187879.732553	36.695655
1534.911567	188165.541627	36.700672
1536.396945	188452.624131	36.705690
1537.485758	188738.313759	36.710708
1539.123987	189033.421907	36.715725
1540.569198	189335.227881	36.720743
1542.252121	189623.349810	36.725760
1543.196308	189923.400908	36.730778
1544.592652	190225.079865	36.735796
1546.302529	190539.428379	36.740813
1547.633549	190853.511081	36.745831
1549.322044	191155.273401	36.750848
1550.692917	191476.334780	36.755866
1552.154290	191793.523713	36.760884
1553.886051	192115.430163	36.765901
1555.330422	192437.157278	36.770919
1556.561829	192758.248430	36.775936
1558.082532	193094.502029	36.780954
1559.598143	193429.285661	36.785972
1561.060545	193755.916921	36.790989
1562.396059	194104.025692	36.796007
1564.171684	194437.883076	36.801024
1565.838928	194778.374380	36.806042
1566.913138	195142.731235	36.811060
1568.536865	195478.383813	36.816077
1570.142761	195838.949694	36.821095
1571.477490	196194.496835	36.826112
1573.174064	196553.223523	36.831130
1574.746827	196917.901533	36.836148
1576.545414	197269.531051	36.841165
1578.023857	197630.610263	36.846183
1579.277852	197994.191518	36.851200
1581.359368	198357.714198	36.856218
1582.940686	198724.051127	36.861236
1584.676484	199086.949243	36.866253
1586.115593	199461.261406	36.871271
1588.048286	199821.655113	36.876288
1589.673345	200177.441961	36.881306
1590.868725	200551.965329	36.886324
1592.908529	200911.750242	36.891341
1594.479358	201283.117530	36.896359
1596.470316	201645.186917	36.901376
1597.976055	202004.735481	36.906394
1599.219641	202377.914652	36.911412
1601.238930	202733.725343	36.916429
1602.909446	203101.949432	36.921447
1604.269851	203463.052838	36.926464
1606.368095	203829.178391	36.931482
1608.014489	204191.863313	36.936500
1609.495307	204555.491535	36.941517
1611.122157	204922.601804	36.946535
1612.042093	205289.995696	36.951552
1614.372084	205659.608984	36.956570
1615.742519	206022.868827	36.961588
1617.750721	206390.862725	36.966605
1619.333668	206756.389117	36.971623
1620.677064	207111.367044	36.976640
1622.667405	207492.549084	36.981658
1624.441675	207855.395147	36.986676
1626.101466	208204.002242	36.991693
1627.512059	208568.714668	36.996711
1629.251883	208939.647058	37.001728
1631.121524	209293.404856	37.006746
1632.324559	209664.924406	37.011764
1634.542114	210018.196090	37.016781
1635.863777	210383.096284	37.021799
1637.661697	210740.859240	37.026816
1639.504029	211095.543411	37.031834
1641.211005	211459.013163	37.036852
1642.637618	211793.553363	37.041869
1643.897539	212125.633519	37.046887
1645.240609	212476.545533	37.051904
1647.103438	212810.966758	37.056922
1648.471472	213162.791647	37.061940
1650.018165	213500.162919	37.066957
1651.974176	213858.674389	37.071975
1653.270635	214207.797681	37.076992
1655.090060	214556.734320	37.082010
1655.951078	214924.624647	37.087028
1657.915842	215283.521172	37.092045
1659.808926	215660.259996	37.097063
1661.043524	216024.029295	37.102080
1662.770423	216380.429496	37.107098
1664.040102	216765.656910	37.112116
1665.720092	217146.043252	37.117133
1667.310520	217523.220307	37.122151
1668.531609	217907.926862	37.127168
1670.456266	218300.671509	37.132186
1671.855764	218701.123937	37.137204
1673.681206	219091.373592	37.142221
1675.448415	219499.641910	37.147239
1676.997746	219897.585171	37.152256
1678.993583	220293.576671	37.157274
1680.424182	220699.060583	37.162292
1682.105750	221103.539408	37.167309
1684.095554	221503.650987	37.172327
1685.720314	221912.688614	37.177344
1687.883424	222314.120654	37.182362
1689.301641	222729.875382	37.187380
1691.169464	223137.581953	37.192397
1692.675843	223539.685592	37.197415
1694.192887	223952.532876	37.202432
1696.450584	224357.029777	37.207450
1697.784506	224812.835730	37.212468
1699.530806	225262.250726	37.217485
1701.355123	225669.287400	37.222503
1702.865396	226083.032088	37.227520
1704.775990	226494.400608	37.232538
1706.547264	226927.790030	37.237556
1708.483023	227330.089219	37.242573
1710.120029	227749.101621	37.247591
1711.724763	228168.171483	37.252608
1713.507923	228579.059624	37.257626
1714.876022	229004.241889	37.262644
1716.635436	229428.878218	37.267661
1718.497107	229861.119166	37.272679
1720.846974	230273.239556	37.277696
1722.415703	230689.884505	37.282714
1723.865863	231119.098298	37.287732
1725.694339	231536.464768	37.292749
1727.811022	231957.518751	37.297767
1729.302154	232371.463289	37.302784
1730.954383	232781.343524	37.307802
1732.817742	233214.228926	37.312820
1734.515753	233628.091784	37.317837
1736.196780	234054.151182	37.322855
1737.678590	234483.902393	37.327872
1739.976623	234898.456757	37.332890
1741.763598	235326.483186	37.337908
1743.277519	235741.600906	37.342925
1745.129603	236167.383271	37.347943
1746.842757	236585.238819	37.352960
1748.870142	236997.353395	37.357978
1750.436814	237418.842065	37.362996
1752.184586	237838.955443	37.368013
1753.783717	238258.814848	37.373031
1755.872184	238674.682393	37.378048
1757.693697	239073.473849	37.383066
1759.048312	239473.384673	37.388084
1760.478951	239862.309936	37.393101
1762.843490	240262.360247	37.398119
1764.231981	240668.897663	37.403136
1765.952417	241057.421522	37.408154
1767.634262	241460.736595	37.413172
1769.507851	241864.579537	37.418189
1771.312074	242279.256061	37.423207
1772.651072	242692.155728	37.428224
1775.286863	243094.477636	37.433242
1776.567473	243509.522064	37.438260
1777.894341	243927.582404	37.443277
1779.556423	244340.736098	37.448295
1781.186318	244768.730888	37.453312
1782.498625	245205.288674	37.458330
1784.541298	245633.648373	37.463348
1786.429504	246079.181071	37.468365
1788.561108	246514.970291	37.473383
1790.016219	246954.656835	37.478400
1791.798704	247392.892704	37.483418
1793.609151	247835.163551	37.488436
1795.207591	248281.127959	37.493453
1797.467589	248726.754984	37.498471
1798.794593	249176.829695	37.503488
1800.816617	249631.006994	37.508506
1802.260642	250085.127791	37.513524
1804.152846	250549.895110	37.518541
1806.368074	251002.009558	37.523559
1808.151389	251467.989630	37.528576
1810.142480	251925.882966	37.533594
1811.884361	252387.933121	37.538612
1813.551071	252842.629089	37.543629
1815.510478	253301.417736	37.548647
1817.195166	253773.029856	37.553664
1819.110675	254232.105723	37.558682
1820.804478	254698.153523	37.563700
1823.085420	255173.300549	37.568717
1824.947822	255640.032196	37.573735
1826.472975	256107.048329	37.578752
1828.429533	256575.085693	37.583770
1830.426781	257050.381792	37.588788
1832.278827	257519.198715	37.593805
1833.749080	257988.129558	37.598823
1835.265749	258475.063714	37.603840
1837.434002	258952.491050	37.608858
1839.112819	259429.592745	37.613876
1841.095661	259919.218822	37.618893
1843.081803	260390.934956	37.623911
1844.651486	260883.525066	37.628928
1846.768964	261358.496313	37.633946
1848.525122	261841.173466	37.638964
1850.357288	262324.193531	37.643981
1852.505402	262804.773303	37.648999
1854.316980	263298.338666	37.654016
1856.154435	263776.505125	37.659034
1857.794948	264262.502605	37.664052
1859.927996	264744.912782	37.669069
1862.329203	265220.775115	37.674087
1863.830360	265708.064720	37.679104
1865.830091	266191.080063	37.684122
1868.056943	266665.750653	37.689140
1869.623132	267146.398016	37.694157
1871.777274	267627.405057	37.699175
1873.234361	268103.598515	37.704192
1875.478736	268566.909130	37.709210
1877.506661	269055.861162	37.714228
1878.995940	269526.433601	37.719245
1881.035104	269982.155556	37.724263
1882.422648	270445.580000	37.729280
1884.317540	270898.835115	37.734298
1886.087906	271356.479461	37.739316
1887.545510	271820.042842	37.744333
1889.532558	272280.952425	37.749351
1891.260178	272758.873134	37.754368
1893.121604	273224.171248	37.759386
1894.664198	273712.307372	37.764404
1896.213433	274187.587828	37.769421
1898.529681	274672.114291	37.774439
1900.126426	275167.630899	37.779456
1901.890450	275658.394043	37.784474
1903.940484	276153.579769	37.789492
1905.298649	276660.157314	37.794509
1907.583461	277164.091290	37.799527
1909.614499	277672.994043	37.804544
1911.583183	278177.790744	37.809562
1913.561524	278687.588837	37.814580
1915.174983	279205.498340	37.819597
1917.397867	279707.175636	37.824615
1918.793351	280231.392701	37.829632
1920.936133	280762.826031	37.834650
1922.936217	281273.223376	37.839668
1924.565686	281811.876295	37.844685
1927.100217	282338.083765	37.849703
1928.343552	282871.691459	37.854720
1930.333258	283405.479036	37.859738
1932.395843	283942.605826	37.864756
1934.215742	284482.869853	37.869773
1935.925575	285028.611453	37.874791
1938.052505	285574.155253	37.879808
1939.885900	286132.065025	37.884826
1941.823598	286685.815139	37.889844
1943.717401	287231.899366	37.894861
1945.720470	287787.996727	37.899879
1947.436451	288349.448004	37.904896
1949.773579	288908.584584	37.909914
1951.997685	289472.157172	37.914932
1953.509095	290035.311638	37.919949
1955.398393	290593.676846	37.924967
1957.659623	291173.111018	37.929984
1959.531884	291738.712997	37.935002
1961.543544	292295.018446	37.940020
1963.635112	292871.373887	37.945037
1965.701419	293433.557771	37.950055
1967.641325	294010.745492	37.955072
1970.016623	294579.146481	37.960090
1971.961764	295135.957437	37.965108
1973.608235	295709.832293	37.970125
1975.799175	296281.353758	37.975143
1977.945625	296846.910848	37.980160
1980.072673	297423.287967	37.985178
1982.481259	297984.604937	37.990196
1984.070399	298542.803184	37.995213
1986.418335	299104.301859	38.000231
1988.331239	299673.183885	38.005248
1990.130797	300232.379366	38.010266
1992.325179	300793.004943	38.015284
1994.533008	301360.126850	38.020301
1996.334899	301914.181917	38.025319
1998.375290	302479.902525	38.030336
2000.674353	303043.799185	38.035354
2002.688873	303593.085287	38.040372
2004.612741	304164.224341	38.045389
2006.946361	304713.831889	38.050407
2008.789218	305275.605815	38.055424
2010.895307	305826.082078	38.060442
2012.959712	306357.489155	38.065460
2014.398913	306891.002447	38.070477
2016.484308	307419.809026	38.075495
2018.119087	307962.171806	38.080512
2019.859313	308501.212197	38.085530
2022.174134	309040.738268	38.090548
2023.753980	309593.638406	38.095565
2025.937597	310132.239206	38.100583
2027.518296	310692.953259	38.105600
2029.156548	311250.073148	38.110618
2031.446154	311809.570162	38.115636
2033.226790	312382.606126	38.120653
2035.370494	312951.540158	38.125671
2037.424427	313521.652826	38.130688
2039.181158	314110.499990	38.135706
2041.476203	314684.804643	38.140724
2043.305062	315283.533945	38.145741
2045.376944	315860.684781	38.150759
2047.139447	316464.671554	38.155776
2049.226267	317061.235735	38.160794
2051.638953	317654.947851	38.165812
2053.282557	318262.519055	38.170829
2055.365948	318867.371489	38.175847
2057.707058	319466.056553	38.180864
2059.559378	320080.178875	38.185882
2061.636130	320684.711326	38.190900
2063.423533	321306.018727	38.195917
2065.587740	321918.498149	38.200935
2067.944234	322548.129455	38.205952
2069.905719	323165.276928	38.210970
2072.216881	323791.729603	38.215988
2074.072120	324420.104741	38.221005
2076.464498	325041.631205	38.226023
2078.881699	325678.304721	38.231040
2080.806013	326315.103727	38.236058
2083.290578	326925.526104	38.241076
2085.115237	327562.506051	38.246093
2086.824171	328184.493784	38.251111
2088.967001	328822.397733	38.256128
2091.246477	329454.509114	38.261146
2093.538936	330084.199610	38.266164
2095.032633	330722.164304	38.271181
2097.766813	331366.669930	38.276199
2100.003887	332005.792102	38.281216
2101.961711	332642.820581	38.286234
2104.483710	333278.352335	38.291252
2106.311286	333919.525416	38.296269
2108.693117	334555.928503	38.301287
2110.617188	335189.251870	38.306304
2112.843270	335827.924813	38.311322
2115.092840	336465.773857	38.316340
2117.244176	337113.607332	38.321357
2119.414572	337743.026297	38.326375
2121.513783	338377.602188	38.331392
2123.660231	339031.225207	38.336410
2125.903835	339655.709589	38.341428
2128.266679	340303.975398	38.346445
2130.307387	340938.528793	38.351463
2132.382645	341565.504546	38.356480
2134.512650	342212.667019	38.361498
2136.925043	342844.697828	38.366516
2138.985429	343484.595820	38.371533
2141.311067	344123.629327	38.376551
2143.440066	344748.397654	38.381568
2145.359656	345384.613267	38.386586
2147.425430	346011.304179	38.391604
2149.816656	346655.089308	38.396621
2151.795085	347285.051390	38.401639
2153.922639	347884.170687	38.406656
2156.339728	348490.238718	38.411674
2159.021799	349083.312198	38.416692
2160.714366	349684.941175	38.421709
2162.805492	350285.049779	38.426727
2164.914971	350877.584955	38.431744
2167.177651	351490.286596	38.436762
2169.168176	352092.468132	38.441780
2171.243673	352705.234410	38.446797
2173.349452	353316.819754	38.451815
2175.685794	353920.999580	38.456832
2177.414312	354534.786720	38.461850
2179.612328	355152.116030	38.466868
2181.652833	355785.930016	38.471885
2183.521865	356412.962612	38.476903
2186.012063	357051.504166	38.481920
2187.610203	357692.415924	38.486938
2189.953532	358327.409787	38.491956
2191.707495	358971.904082	38.496973
2194.236679	359623.643324	38.501991
2196.835875	360272.823362	38.507008
2198.589496	360929.769059	38.512026
2201.156273	361587.736737	38.517044
2203.391364	362246.078031	38.522061
2205.440488	362908.827921	38.527079
2207.936262	363566.672722	38.532096
2209.606473	364232.557654	38.537114
2212.305968	364899.504244	38.542132
2214.282818	365574.244931	38.547149
2216.885616	366237.049190	38.552167
2219.005746	366903.269933	38.557184
2221.295040	367584.138100	38.562202
2223.502998	368265.692169	38.567220
2226.188541	368931.580510	38.572237
2228.608015	369604.323943	38.577255
2230.742411	370276.518710	38.582272
2232.953708	370961.573344	38.587290
2235.510610	371636.057463	38.592308
2237.745898	372305.078241	38.597325
2239.867029	372975.221320	38.602343
2242.156689	373662.544878	38.607360
2244.593477	374337.606481	38.612378
2247.061633	374999.944001	38.617396
2249.561378	375685.012313	38.622413
2251.447764	376353.481352	38.627431
2254.128255	377021.476728	38.632448
2256.084699	377697.084952	38.637466
2258.574508	378364.096625	38.642484
2260.490376	379042.550414	38.647501
2263.051121	379725.093529	38.652519
2265.222962	380396.910164	38.657536
2267.675597	381076.147168	38.662554
2270.063215	381745.213201	38.667572
2272.551573	382426.369058	38.672589
2274.513744	383098.571220	38.677607
2276.831913	383762.435207	38.682624
2279.079370	384441.306920	38.687642
2281.300720	385126.583132	38.692660
2283.719656	385795.028450	38.697677
2286.184646	386481.351036	38.702695
2288.403184	387145.212339	38.707712
2290.829042	387833.261424	38.712730
2292.757344	388491.666411	38.717748
2295.160919	389176.749034	38.722765
2297.658524	389854.703146	38.727783
2299.986669	390524.102368	38.732800
2302.056392	391201.742661	38.737818
2304.437443	391869.405507	38.742836
2306.557274	392524.245661	38.747853
2308.939423	393171.779164	38.752871
2311.247733	393810.110215	38.757888
2313.284853	394458.864293	38.762906
2315.632949	395110.087522	38.767924
2318.145658	395752.880215	38.772941
2319.819502	396409.584677	38.777959
2322.221234	397065.951648	38.782976
2324.586025	397736.324774	38.787994
2326.749960	398405.169771	38.793012
2329.119508	399072.014120	38.798029
2331.406102	399748.461157	38.803047
2333.383782	400426.565089	38.808064
2335.545329	401103.533007	38.813082
2337.886574	401789.248017	38.818100
2340.296522	402491.126681	38.823117
2341.972865	403189.840327	38.828135
2344.273979	403887.065268	38.833152
2346.808757	404598.676355	38.838170
2349.191351	405306.113860	38.843188
2351.457311	406033.187699	38.848205
2353.760074	406744.655241	38.853223
2356.150555	407461.916751	38.858240
2358.266107	408191.440947	38.863258
2360.946040	408921.359066	38.868276
2363.548609	409649.978281	38.873293
2365.654775	410377.899715	38.878311
2368.123716	411114.531314	38.883328
2370.442593	411862.743207	38.888346
2372.803029	412605.531926	38.893364
2375.311471	413342.829600	38.898381
2377.688017	414101.201274	38.903399
2380.338800	414845.069083	38.908416
2382.620807	415591.179860	38.913434
2384.900433	416339.016983	38.918452
2387.693653	417098.777058	38.923469
2390.192395	417851.117810	38.928487
2392.609139	418606.159509	38.933504
2394.631967	419357.977077	38.938522
2397.194736	420120.647632	38.943540
2399.694089	420872.012171	38.948557
2402.115316	421649.396573	38.953575
2404.737113	422396.922199	38.958592
2407.067311	423149.587819	38.963610
2409.228383	423921.550868	38.968628
2411.794883	424682.232417	38.973645
2413.903055	425460.231851	38.978663
2416.525909	426225.514167	38.983680
2418.761154	427007.290999	38.988698
2421.417857	427782.087439	38.993716
2423.755002	428557.114063	38.998733
2426.202049	429338.273634	39.003751
2428.958562	430111.206062	39.008768
2431.636080	430888.580959	39.013786
2433.843830	431653.858848	39.018804
2436.261269	432428.239074	39.023821
2438.756727	433213.969475	39.028839
2441.129630	433990.937090	39.033856
2443.774593	434759.128183	39.038874
2446.175180	435533.761619	39.043892
2448.660268	436306.532945	39.048909
2451.029863	437093.720470	39.053927
2453.644060	437868.947811	39.058944
2456.189902	438643.552570	39.063962
2458.672597	439430.589401	39.068980
2461.246788	440209.790892	39.073997
2463.568695	440983.997431	39.079015
2466.050257	441743.679689	39.084032
2468.306672	442489.914458	39.089050
2470.366565	443235.296254	39.094068
2472.961477	443972.773178	39.099085
2475.388600	444724.114764	39.104103
2478.402680	445473.360568	39.109120
2480.517198	446218.580703	39.114138
2482.346612	446966.553752	39.119156
2485.518677	447722.777309	39.124173
2487.829157	448495.049605	39.129191
2490.201411	449244.016843	39.134208
2492.382098	450000.120801	39.139226
2494.932351	450773.383335	39.144244
2497.433417	451539.848564	39.149261
2499.404613	452330.192975	39.154279
2501.625514	453103.120457	39.159296
2504.290654	453895.162122	39.164314
2506.989884	454689.847909	39.169332
2509.561468	455487.052374	39.174349
2511.974757	456296.791642	39.179367
2514.630627	457094.779210	39.184384
2517.429794	457902.469762	39.189402
2519.666508	458706.125812	39.194420
2522.396888	459502.641278	39.199437
2524.450353	460327.546572	39.204455
2527.273468	461143.292851	39.209472
2529.723531	461959.320052	39.214490
2531.859400	462793.410757	39.219508
2535.206556	463622.110904	39.224525
2537.615486	464459.573728	39.229543
2540.068593	465287.795175	39.234560
2542.921499	466117.987615	39.239578
2545.303012	466957.874770	39.244596
2548.034935	467792.513260	39.249613
2550.263124	468636.446034	39.254631
2553.146597	469474.725938	39.259648
2555.959595	470316.113429	39.264666
2558.209587	471159.274503	39.269684
2561.501425	471985.351670	39.274701
2563.932583	472841.847003	39.279719
2566.312591	473675.376573	39.284736
2568.943714	474519.638080	39.289754
2571.510728	475363.164810	39.294772
2574.413917	476197.202725	39.299789
2576.908583	477050.615457	39.304807
2579.512051	477887.556100	39.309824
2582.476268	478739.651458	39.314842
2584.656802	479580.119967	39.319860
2587.610647	480423.654162	39.324877
2590.418479	481265.557358	39.329895
2592.946319	482107.871534	39.334912
2595.755683	482953.129470	39.339930
2598.214330	483798.102531	39.344948
2601.074924	484635.699114	39.349965
2603.209524	485484.230472	39.354983
2606.066729	486328.260524	39.360000
2608.675189	487168.555749	39.365018
2611.479738	488023.720108	39.370036
2614.001181	488860.314398	39.375053
2616.243239	489713.167174	39.380071
2618.771557	490557.300446	39.385088
2621.314214	491410.878352	39.390106
2623.748019	492261.353642	39.395124
2626.847547	493124.999458	39.400141
2629.095297	493988.035845	39.405159
2631.817424	494841.766987	39.410176
2634.287193	495698.625208	39.415194
2636.953696	496567.314656	39.420212
2639.575719	497407.109011	39.425229
2642.265281	498248.313336	39.430247
2644.687271	499065.457028	39.435264
2647.287765	499892.266878	39.440282
2649.606097	500717.266367	39.445300
2652.733024	501542.898486	39.450317
2655.658530	502380.627170	39.455335
2657.837955	503203.306409	39.460352
2660.723536	504031.879635	39.465370
2663.079659	504870.936842	39.470388
2665.579785	505701.657369	39.475405
2668.171409	506549.010293	39.480423
2670.705561	507402.681301	39.485440
2673.209829	508264.933463	39.490458
2675.731244	509117.154447	39.495476
2678.354263	509983.832015	39.500493
2681.001466	510857.364619	39.505511
2683.415340	511733.912135	39.510528
2686.328771	512612.344934	39.515546
2689.173687	513500.064335	39.520564
2691.830787	514381.616083	39.525581
2694.309658	515279.727678	39.530599
2696.852293	516173.493796	39.535616
2700.147377	517070.057468	39.540634
2702.800941	517981.287178	39.545652
2705.653835	518865.072083	39.550669
2708.491098	519769.716778	39.555687
2710.834601	520685.774903	39.560704
2713.960882	521582.909722	39.565722
2716.227946	522496.806409	39.570740
2719.759283	523410.137351	39.575757
2722.283899	524327.910605	39.580775
2724.982911	525246.807911	39.585792
2727.885251	526158.011207	39.590810
2730.625598	527075.228482	39.595828
2733.417515	527994.294250	39.600845
2736.062402	528921.484113	39.605863
2738.928707	529849.082863	39.610880
2741.830376	530764.686012	39.615898
2744.385659	531701.482605	39.620916
2747.349560	532624.762192	39.625933
2749.871897	533551.025914	39.630951
2752.766787	534492.016808	39.635968
2755.578470	535429.991005	39.640986
2758.231428	536357.312037	39.646004
2760.814004	537296.209091	39.651021
2764.060779	538251.640613	39.656039
2766.240300	539186.404446	39.661056
2769.380115	540115.414336	39.666074
2772.469250	541073.499939	39.671092
2775.182015	542015.938061	39.676109
2777.843686	542963.251076	39.681127
2780.518162	543901.947491	39.686144
2783.588170	544844.991893	39.691162
2786.305692	545797.435025	39.696180
2789.274816	546756.057299	39.701197
2791.918466	547699.179480	39.706215
2794.904472	548656.410100	39.711232
2797.915595	549585.414893	39.716250
2800.753173	550536.053218	39.721268
2803.694314	551478.062414	39.726285
2806.679312	552421.657992	39.731303
2809.514398	553361.442945	39.736320
2812.160230	554293.453833	39.741338
2814.822514	555236.453892	39.746356
2817.952499	556180.466435	39.751373
2820.654987	557112.674406	39.756391
2822.829210	558061.837088	39.761408
2826.524779	558979.279987	39.766426
2828.868603	559902.056856	39.771444
2831.784964	560796.292118	39.776461
2834.566998	561689.333498	39.781479
2837.616218	562607.384160	39.786496
2840.285712	563496.302768	39.791514
2842.993200	564401.526684	39.796532
2845.678278	565311.110466	39.801549
2848.475453	566216.845908	39.806567
2850.851981	567130.420124	39.811584
2853.692192	568047.668861	39.816602
2856.560867	568980.109260	39.821620
2859.226924	569911.962986	39.826637
2862.028455	570839.108319	39.831655
2864.777159	571782.156002	39.836672
2867.625547	572728.831104	39.841690
2869.980227	573683.997989	39.846708
2872.947632	574640.948526	39.851725
2875.880690	575603.000092	39.856743
2878.426883	576574.323610	39.861760
2881.636721	577549.174657	39.866778
2884.351807	578536.973580	39.871796
2887.119117	579517.110858	39.876813
2890.106772	580505.610697	39.881831
2892.840232	581501.044468	39.886848
2896.029125	582500.535003	39.891866
2898.891162	583507.218724	39.896884
2901.477737	584510.204525	39.901901
2904.748018	585520.866361	39.906919
2907.487690	586532.183144	39.911936
2910.948392	587540.589456	39.916954
2913.870505	588571.455756	39.921972
2916.533892	589585.886994	39.926989
2919.662363	590607.372184	39.932007
2922.782576	591636.939370	39.937024
2925.597027	592659.502919	39.942042
2928.514042	593688.374431	39.947060
2931.129033	594721.915328	39.952077
2934.146210	595753.696155	39.957095
2936.988282	596790.774669	39.962112
2939.888179	597831.207526	39.967130
2943.009358	598877.570745	39.972148
2945.741281	599928.160338	39.977165
2949.055747	600977.557128	39.982183
2952.000427	602038.184470	39.987200
2955.020086	603088.038416	39.992218
2957.896447	604142.675429	39.997236
2961.298660	605200.782267	40.002253
2964.449593	606241.465475	40.007271
2967.142442	607304.398246	40.012288
2970.553396	608354.002578	40.017306
2973.400907	609414.409535	40.022324
2976.125054	610459.427774	40.027341
2979.212712	611513.743352	40.032359
2982.174003	612589.688991	40.037376
2985.754977	613635.169237	40.042394
2988.304666	614696.724423	40.047412
2991.461232	615747.226453	40.052429
2994.548325	616797.589872	40.057447
2997.282935	617869.159452	40.062464
3000.627956	618919.027349	40.067482
3003.499091	619979.069730	40.072500
3006.492822	621040.638112	40.077517
3009.501325	622097.302482	40.082535
3012.539863	623153.209089	40.087552
3015.911695	624208.008022	40.092570
3018.761625	625276.828873	40.097588
3021.670468	626328.248307	40.102605
3025.080114	627364.096448	40.107623
3027.908199	628388.551736	40.112640
3030.999042	629396.383825	40.117658
3033.985713	630407.582904	40.122676
3036.622557	631416.995170	40.127693
3039.993950	632417.851532	40.132711
3042.715748	633423.761855	40.137728
3045.913430	634441.876934	40.142746
3048.742676	635460.552406	40.147764
3051.504414	636490.019461	40.152781
3054.568107	637508.156105	40.157799
3057.431286	638546.833935	40.162816
3060.018013	639583.706470	40.167834
3063.391351	640627.329264	40.172852
3066.515353	641677.122422	40.177869
3069.469258	642719.703170	40.182887
3072.598540	643791.922896	40.187904
3075.715705	644849.320360	40.192922
3078.215131	645915.734532	40.197940
3081.313078	647002.129861	40.202957
3084.519771	648068.100175	40.207975
3087.094654	649156.891427	40.212992
3089.919217	650253.547609	40.218010
3093.260594	651363.154809	40.223028
3096.318200	652472.884361	40.228045
3099.606189	653580.458792	40.233063
3102.502716	654697.638630	40.238080
3105.441565	655822.107115	40.243098
3108.901282	656947.456859	40.248116
3111.697853	658071.989821	40.253133
3115.267972	659210.308366	40.258151
3118.040983	660350.118936	40.263168
3121.106316	661486.561278	40.268186
3124.410127	662630.895002	40.273204
3127.362406	663778.834110	40.278221
3130.650939	664930.960249	40.283239
3134.108818	666093.568817	40.288256
3136.866261	667248.986726	40.293274
3140.366637	668413.096820	40.298292
3143.388863	669583.161881	40.303309
3146.915101	670736.785200	40.308327
3150.240582	671909.397032	40.313344
3153.117735	673072.787395	40.318362
3156.397546	674229.205461	40.323380
3159.075377	675413.368599	40.328397
3162.526304	676578.713791	40.333415
3165.729739	677763.137506	40.338432
3169.224606	678941.150161	40.343450
3172.695750	680122.742937	40.348468
3175.615440	681296.077750	40.353485
3179.144110	682476.414560	40.358503
3182.324742	683654.570443	40.363520
3185.388794	684834.281849	40.368538
3188.904937	686006.367203	40.373556
3192.082202	687184.463579	40.378573
3195.111369	688353.346422	40.383591
3198.311363	689532.671401	40.388608
3201.764148	690719.194553	40.393626
3204.759935	691885.687818	40.398644
3208.014590	693065.779147	40.403661
3211.323778	694253.096779	40.408679
3214.084584	695433.302459	40.413696
3217.506445	696618.548523	40.418714
3220.728991	697812.990905	40.423732
3223.744697	698996.149201	40.428749
3226.988138	700185.505570	40.433767
3230.003275	701381.132129	40.438784
3232.882560	702566.159538	40.443802
3236.463886	703740.750857	40.448820
3239.342568	704911.632158	40.453837
3242.535200	706062.486316	40.458855
3245.696899	707206.999914	40.463872
3248.558114	708365.971959	40.468890
3252.229326	709519.156759	40.473908
3255.050579	710685.893075	40.478925
3258.769854	711847.172673	40.483943
3261.568832	713007.554079	40.488960
3264.543710	714184.773680	40.493978
3267.993291	715352.793599	40.498996
3270.862275	716552.464384	40.504013
3273.918670	717738.871752	40.509031
3277.280296	718941.335184	40.514048
3280.317512	720146.300147	40.519066
3283.713648	721352.020492	40.524084
3286.784586	722582.885610	40.529101
3290.185646	723791.809986	40.534119
3293.262739	725031.801110	40.539136
3296.539689	726259.562514	40.544154
3300.026052	727491.206993	40.549172
3303.211121	728739.711851	40.554189
3306.435868	729995.231318	40.559207
3309.841460	731253.045961	40.564224
3313.161475	732517.692018	40.569242
3316.559969	733769.288979	40.574260
3319.995933	735039.396222	40.579277
3323.283740	736313.226445	40.584295
3326.599845	737586.602441	40.589312
3329.987607	738864.105799	40.594330
3333.617497	740140.574636	40.599348
3336.406251	741428.618444	40.604365
3339.588311	742722.108919	40.609383
3343.014525	744021.264507	40.614400
3346.453742	745318.428124	40.619418
3350.231432	746623.504492	40.624436
3353.110776	747942.114531	40.629453
3356.538791	749242.669784	40.634471
3360.184643	750560.512170	40.639488
3363.514142	751870.694086	40.644506
3366.681833	753187.969957	40.649524
3370.220014	754514.808560	40.654541
3373.580635	755840.068096	40.659559
3377.507018	757165.447674	40.664576
3380.232321	758488.333528	40.669594
3383.944757	759806.544852	40.674612
3387.216948	761156.335962	40.679629
3390.863883	762489.146783	40.684647
3394.185876	763814.200370	40.689664
3397.032044	765158.277797	40.694682
3400.788300	766495.129298	40.699700
3404.295712	767837.140623	40.704717
3407.549830	769179.639579	40.709735
3411.384412	770527.500278	40.714752
3414.583296	771872.910595	40.719770
3418.248345	773222.419622	40.724788
3421.434200	774562.771524	40.729805
3424.774083	775909.138352	40.734823
3428.126240	777261.784817	40.739840
3431.188840	778616.731121	40.744858
3434.888337	779964.252121	40.749876
3438.391884	781322.006281	40.754893
3441.591267	782680.732416	40.759911
3445.292257	784047.605046	40.764928
3448.333108	785416.287492	40.769946
3451.640024	786772.013634	40.774964
3455.061762	788156.092417	40.779981
3458.372267	789514.138743	40.784999
3461.694252	790871.344258	40.790004
3464.978691	792182.292977	40.795008
3468.730478	793438.505110	40.800013
3471.323280	794655.695645	40.805018
3474.704877	795792.716415	40.810023
3477.924425	796872.097488	40.815028
3480.738841	797874.273080	40.820032
3483.654649	798801.597378	40.825037
3486.119423	799678.774068	40.830042
3488.968853	800473.401505	40.835047
3491.505693	801213.781489	40.840052
3493.586047	801890.340856	40.845056
3496.014099	802488.104337	40.850061
3498.015687	803034.978797	40.855066
3500.015240	803531.102559	40.860071
3502.449862	803975.728038	40.865076
3503.958366	804345.111632	40.870080
3505.731234	804672.166155	40.875085
3507.315197	804950.451320	40.880090
3508.862908	805178.869289	40.885095
3510.171930	805373.196140	40.890100
3511.293426	805516.316254	40.895104
3512.944568	805620.076891	40.900109
3514.076236	805689.359082	40.905114
3514.667226	805717.745145	40.910119
3515.725390	805720.120126	40.915124
3516.749885	805696.125347	40.920128
3518.108137	805631.776830	40.925133
3518.559060	805540.956170	40.930138
3519.235180	805427.642991	40.935143
3519.985187	805285.977779	40.940148
3520.278855	805138.550399	40.945152
3520.793113	804947.201629	40.950157
3521.332541	804754.617584	40.955162
3521.866160	804536.875145	40.960167
3522.500392	804302.535481	40.965172
3522.864772	804055.482787	40.970176
3523.871348	803791.887541	40.975181
3523.562899	803518.641740	40.980186
3523.751065	803230.639574	40.985191
3524.320541	802936.039604	40.990196
3524.322761	802629.994518	40.995200
3524.919303	802313.979074	41.000205
3524.959818	801989.751092	41.005210
3525.053388	801656.326098	41.010215
3525.302117	801306.278474	41.015220
3525.285168	800958.415461	41.020224
3525.600654	800608.125234	41.025229
3525.618974	800256.786831	41.030234
3525.448900	799881.321082	41.035239
3525.477694	799516.401089	41.040244
3525.628597	799142.805193	41.045248
3526.023733	798768.167462	41.050253
3525.872538	798378.140338	41.055258
3525.962100	797991.683546	41.060263
3526.008678	797610.267845	41.065268
3525.558318	797225.820766	41.070272
3525.735334	796834.867694	41.075277
3525.939631	796443.397306	41.080282
3525.911797	796046.395668	41.085287
3525.733575	795652.587489	41.090292
3525.621463	795253.639951	41.095296
3525.846691	794851.029663	41.100301
3525.731185	794456.898344	41.105306
3525.321136	794053.512121	41.110311
3525.714512	793651.492739	41.115316
3525.564971	793253.419716	41.120320
3525.504522	792848.040344	41.125325
3525.193875	792448.180106	41.130330
3525.311201	792034.030573	41.135335
3525.153543	791647.608046	41.140340
3524.726960	791237.283874	41.145344
3525.008915	790836.890706	41.150349
3524.763872	790459.113465	41.155354
3524.796234	790060.387940	41.160359
3524.738903	789656.495252	41.165364
3524.554458	789259.725879	41.170368
3524.430457	788856.928841	41.175373
3524.464937	788463.813779	41.180378
3524.342050	788072.717991	41.185383
3524.042035	787673.421549	41.190388
3523.862122	787284.159552	41.195392
3523.707001	786889.661543	41.200397
3523.789040	786499.920279	41.205402
3523.706723	786119.525658	41.210407
3523.979019	785723.319532	41.215412
3523.681053	785347.049169	41.220416
3523.479684	784953.730159	41.225421
3522.941587	784564.477205	41.230426
3523.173479	784178.223476	41.235431
3522.988047	783798.312530	41.240436
3522.442199	783419.178565	41.245440
3522.312480	783055.104520	41.250445
3522.400353	782679.712607	41.255450
3522.109874	782302.887790	41.260455
3522.043097	781938.796069	41.265460
3521.631476	781583.892756	41.270464
3521.858003	781210.664337	41.275469
3521.715377	780853.417753	41.280474
3521.095995	780492.984794	41.285479
3521.259191	780142.245578	41.290484
3520.872910	779789.119612	41.295488
3520.921073	779436.347713	41.300493
3520.760804	779088.858502	41.305498
3520.540906	778753.025882	41.310503
3520.763785	778405.243950	41.315508
3520.302352	778063.464204	41.320512
3520.371079	777704.354123	41.325517
3520.233612	777371.298803	41.330522
3519.978499	777038.542975	41.335527
3520.093326	776699.705352	41.340532
3519.553610	776373.365496	41.345536
3519.512379	776039.150406	41.350541
3519.440993	775709.159050	41.355546
3519.207461	775368.199984	41.360551
3519.145881	775047.187233	41.365556
3519.135163	774726.496701	41.370560
3519.074123	774398.463350	41.375565
3518.753924	774079.765183	41.380570
3518.569424	773771.618767	41.385575
3518.809736	773452.604020	41.390580
3518.436191	773134.415320	41.395584
3518.373469	772817.097431	41.400589
3518.180930	772518.848832	41.405594
3518.086794	772206.681533	41.410599
3517.924803	771896.433280	41.415604
3517.547788	771596.897007	41.420608
3517.611587	771294.566479	41.425613
3517.262696	771008.253371	41.430618
3517.168111	770717.995191	41.435623
3517.047423	770427.779179	41.440628
3517.006168	770138.671914	41.445632
3517.135876	769848.145556	41.450637
3516.687628	769562.187000	41.455642
3516.312465	769269.651609	41.460647
3516.750185	768999.589447	41.465652
3516.163871	768712.881702	41.470656
3516.272383	768429.005315	41.475661
3516.023456	768163.313399	41.480666
3516.205826	767892.908087	41.485671
3516.188036	767615.921428	41.490676
3515.624799	767337.683523	41.495680
3515.715037	767074.312001	41.500685
3515.341962	766816.824040	41.505690
3515.255511	766545.921187	41.510695
3515.272623	766284.949259	41.515700
3515.180805	766039.810749	41.520704
3515.159334	765780.158577	41.525709
3514.654672	765519.295165	41.530714
3514.695236	765267.848270	41.535719
3515.087038	765021.314807	41.540724
3514.720821	764781.850280	41.545728
3514.705109	764522.942426	41.550733
3514.098142	764279.310340	41.555738
3514.059579	764032.174226	41.560743
3514.123462	763795.023543	41.565748
3513.707756	763566.229150	41.570752
3514.046925	763323.692310	41.575757
3513.742234	763086.678624	41.580762
3513.741768	762857.892882	41.585767
3513.838791	762629.626644	41.590772
3513.657445	762401.300707	41.595776
3513.629974	762171.314829	41.600781
3513.499902	761932.559041	41.605786
3513.243865	761706.394641	41.610791
3513.545016	761483.584591	41.615796
3513.229152	761266.443819	41.620800
3513.047487	761040.888498	41.625805
3513.108026	760822.193018	41.630810
3512.934598	760588.729722	41.635815
3512.661789	760374.269558	41.640820
3512.582966	760170.181305	41.645824
3512.546386	759954.979628	41.650829
3512.344538	759744.338259	41.655834
3512.133676	759537.886450	41.660839
3512.434034	759324.436945	41.665844
3511.978390	759121.566737	41.670848
3511.924563	758905.400590	41.675853
3511.763252	758703.210868	41.680858
3511.268401	758504.574363	41.685863
3511.624351	758315.612798	41.690868
3511.169354	758119.279024	41.695872
3511.383781	757921.102602	41.700877
3511.556925	757739.115309	41.705882
3511.161405	757551.591095	41.710887
3511.444625	757360.841096	41.715892
3511.277985	757169.666888	41.720896
3511.001927	756988.870870	41.725901
3510.519779	756807.561581	41.730906
3510.468818	756621.339728	41.735911
3510.686926	756441.090975	41.740916
3510.750851	756272.117812	41.745920
3510.153507	756085.133760	41.750925
3510.203553	755915.315826	41.755930
3510.302958	755746.127731	41.760935
3510.408153	755558.373293	41.765940
3509.932569	755396.183455	41.770944
3510.061032	755229.003194	41.775949
3509.966141	755057.758428	41.780954
3509.702096	754900.558908	41.785959
3509.865295	754729.066789	41.790964
3509.700579	754569.918632	41.795968
3509.883200	754410.463074	41.800973
3509.964886	754242.330905	41.805978
3509.541234	754080.795907	41.810983
3509.783832	753917.962691	41.815988
3509.356720	753763.630585	41.820992
3509.685714	753608.973280	41.825997
3509.656924	753450.865859	41.831002
3509.247620	753284.571296	41.836007
3509.442924	753128.099262	41.841012
3509.043336	752973.203548	41.846016
3509.344964	752829.646205	41.851021
3509.285478	752663.527500	41.856026
3508.927396	752519.529843	41.861031
3509.004252	752364.592769	41.866036
3508.809107	752223.476546	41.871040
3509.069401	752079.862662	41.876045
3508.871798	751926.147325	41.881050
3508.898166	751779.800588	41.886055
3508.835408	751623.538094	41.891060
3508.531834	751484.451266	41.896064
3508.393310	751334.270652	41.901069
3508.507020	751208.051119	41.906074
3508.215370	751068.856054	41.911079
3508.442618	750929.276610	41.916084
3508.128169	750798.181345	41.921088
3508.178336	750645.486426	41.926093
3508.098641	750518.151355	41.931098
3507.955892	750389.392000	41.936103
3508.240885	750254.385007	41.941108
3507.459831	750136.841651	41.946112
3507.767657	750003.802566	41.951117
3507.982161	749877.001303	41.956122
3507.770249	749760.642928	41.961127
3508.082336	749625.719332	41.966132
3507.524085	749499.681479	41.971136
3507.495090	749370.293590	41.976141
3507.817687	749251.764470	41.981146
3507.540003	749116.879798	41.986151
3507.948529	748993.194203	41.991156
3507.392311	748883.994191	41.996160
3507.557875	748753.971072	42.001165
3507.483607	748641.921302	42.006170
3507.065655	748521.724292	42.011175
3507.282460	748403.842021	42.016180
3507.247853	748290.792418	42.021184
3507.034786	748159.537020	42.026189
3507.210973	748054.553064	42.031194
3507.381975	747939.142012	42.036199
3507.311545	747831.724942	42.041204
3506.992744	747712.783902	42.046208
3507.127289	747593.519263	42.051213
3507.347266	747479.971191	42.056218
3507.158360	747364.017911	42.061223
3507.287093	747258.783964	42.066228
3506.993879	747144.821378	42.071232
3506.893951	747031.171225	42.076237
3506.712185	746920.399339	42.081242
3506.515904	746810.073071	42.086247
3506.718953	746692.463723	42.091252
3506.663222	746597.382919	42.096256
3506.726333	746490.370186	42.101261
3506.515350	746390.567733	42.106266
3506.254409	746283.210159	42.111271
3506.679519	746170.301202	42.116276
3506.687225	746087.164844	42.121280
3506.551255	745971.972996	42.126285
3506.786913	745874.166309	42.131290
3506.553367	745759.580547	42.136295
3506.602959	745660.318986	42.141300
3506.352990	745569.310890	42.146304
3506.551907	745457.961259	42.151309
3506.536604	745355.493539	42.156314
3506.325090	745254.539764	42.161319
3506.639605	745147.269517	42.166324
3506.284492	745049.401578	42.171328
3505.938585	744944.115828	42.176333
3505.961361	744852.510694	42.181338
3505.732901	744753.728374	42.186343
3505.981909	744658.870426	42.191348
3505.870974	744569.409750	42.196352
3505.965628	744474.673882	42.201357
3506.002827	744384.395701	42.206362
3505.799144	744299.001088	42.211367
3506.182054	744208.565049	42.216372
3505.813361	744106.139239	42.221376
3506.133977	744015.414609	42.226381
3505.971233	743932.629570	42.231386
3505.636080	743847.943878	42.236391
3505.802214	743745.128596	42.241396
3505.628570	743667.435020	42.246400
3505.564727	743564.408059	42.251405
3505.553771	743487.674752	42.256410
3505.770551	743393.004615	42.261415
3505.526703	743306.765299	42.266420
3505.071388	743230.794922	42.271424
3505.397398	743148.217764	42.276429
3505.579790	743071.695771	42.281434
3505.275635	742983.138903	42.286439
3505.274204	742905.359982	42.291444
3505.384130	742835.473485	42.296448
3505.412084	742750.716155	42.301453
3505.441057	742671.594833	42.306458
3505.171328	742598.455766	42.311463
3505.466884	742505.542139	42.316468
3505.197200	742422.214896	42.321472
3505.132647	742342.462837	42.326477
3505.464124	742275.106280	42.331482
3504.880479	742199.987765	42.336487
3505.330426	742116.687076	42.341492
3504.893972	742037.932798	42.346496
3505.106473	741956.598176	42.351501
3504.984279	741885.505198	42.356506
3504.955143	741809.549804	42.361511
3505.267005	741733.389131	42.366516
3505.072730	741664.432562	42.371520
3505.113406	741586.188614	42.376525
3505.373887	741523.238836	42.381530
3504.980803	741444.718771	42.386535
3505.234009	741364.063730	42.391540
3505.134327	741287.917122	42.396544
3505.025268	741204.105449	42.401549
3505.167808	741127.571187	42.406554
3504.854659	741049.380230	42.411559
3505.097746	740975.894347	42.416564
3504.930882	740912.416619	42.421568
3504.746511	740835.636645	42.426573
3505.069258	740761.591594	42.431578
3504.995766	740702.894427	42.436583
3504.976275	740622.771373	42.441588
3504.689420	740551.100000	42.446592
3504.941861	740484.334763	42.451597
3504.906576	740404.311026	42.456602
3504.502819	740334.783837	42.461607
3504.795498	740267.119813	42.466612
3504.889356	740200.032070	42.471616
3505.044589	740117.649262	42.476621
3504.769739	740055.864243	42.481626
3504.679972	739975.795694	42.486631
3504.821376	739902.613411	42.491636
3504.625140	739840.220174	42.496640
3504.641590	739769.629475	42.501645
3504.616065	739700.281731	42.506650
3504.625240	739639.732806	42.511655
3504.964846	739570.175364	42.516660
3504.755135	739509.265771	42.521664
3504.418086	739443.133055	42.526669
3504.609504	739383.294172	42.531674
3504.452027	739320.939937	42.536679
3504.892800	739258.387700	42.541684
3505.278065	739184.614460	42.546688
3504.733232	739111.092729	42.551693
3504.949048	739044.321424	42.556698
3504.508557	738972.017982	42.561703
3504.692370	738907.378064	42.566708
3504.512184	738848.091101	42.571712
3504.376083	738778.159868	42.576717
3503.870363	738713.285679	42.581722
3504.269084	738658.948147	42.586727
3504.344249	738591.454122	42.591732
3504.183327	738543.788000	42.596736
3504.475667	738479.571992	42.601741
3504.562841	738414.449253	42.606746
3504.171125	738357.370373	42.611751
3504.196462	738297.798072	42.616756
3504.355919	738245.575113	42.621760
3504.254299	738177.265620	42.626765
3504.677830	738118.962228	42.631770
3504.305653	738059.701027	42.636775
3504.400235	737990.862840	42.641780
3504.222914	737934.091941	42.646784
3504.211074	737866.210288	42.651789
3503.981107	737800.738966	42.656794
3503.720786	737748.285047	42.661799
3504.218425	737686.403810	42.666804
3504.164583	737636.784929	42.671808
3504.070903	737584.846753	42.676813
3504.266057	737524.894338	42.681818
3504.125959	737467.223339	42.686823
3504.164040	737405.316685	42.691828
3504.333356	737348.929835	42.696832
3503.963728	737302.131858	42.701837
3504.113814	737245.500038	42.706842
3504.036872	737193.012252	42.711847
3504.249428	737115.834058	42.716852
3504.276897	737063.476666	42.721856
3504.001450	737014.682162	42.726861
3504.150749	736952.060904	42.731866
3504.135608	736890.159029	42.736871
3504.420791	736830.582446	42.741876
3504.297607	736779.930493	42.746880
3504.143127	736722.503910	42.751885
3504.292376	736657.999922	42.756890
3504.054394	736604.347152	42.761895
3504.260522	736545.721707	42.766900
3503.692513	736492.963833	42.771904
3504.117291	736431.134380	42.776909
3503.981851	736383.055254	42.781914
3503.766132	736324.398721	42.786919
3504.029561	736262.198649	42.791924
3503.699674	736212.319480	42.796929
3503.928092	736164.970905	42.801933
3503.901051	736106.083729	42.806938
3503.455953	736060.033244	42.811943
3503.881581	735998.546738	42.816948
3503.578058	735958.015177	42.821953
3503.682937	735905.241533	42.826957
3504.016294	735859.507041	42.831962
3503.642276	735805.326931	42.836967
3503.769797	735761.011536	42.841972
3503.861940	735716.107829	42.846977
3503.539297	735666.026095	42.851981
3503.817936	735621.586047	42.856986
3503.573154	735572.035309	42.861991
3503.919649	735513.577155	42.866996
3503.631946	735468.338707	42.872001
3503.452238	735423.676127	42.877005
3503.664516	735362.912810	42.882010
3503.662361	735326.386868	42.887015
3503.627515	735268.880654	42.892020
3503.447046	735219.168655	42.897025
3503.827233	735180.500284	42.902029
3503.604503	735119.410843	42.907034
3503.343407	735082.827467	42.912039
3503.763272	735023.215264	42.917044
3503.439666	734989.611502	42.922049
3503.360744	734935.228400	42.927053
3503.561370	734899.954007	42.932058
3503.848036	734854.122491	42.937063
3503.744279	734807.662086	42.942068
3503.248823	734764.136793	42.947073
3503.346108	734719.276161	42.952077
3503.605000	734667.211464	42.957082
3503.193690	734631.343750	42.962087
3503.285903	734572.623661	42.967092
3503.435271	734536.663142	42.972097
3503.430676	734489.145084	42.977101
3503.590033	734445.559670	42.982106
3503.295178	734402.345857	42.987111
3503.149335	734350.444797	42.992116
3503.260883	734318.251518	42.997121
3503.436889	734265.108876	43.002125
3503.286930	734231.522829	43.007130
3503.470592	734198.772684	43.012135
3503.847295	734145.794190	43.017140
3503.495538	734109.468823	43.022145
3503.367009	734065.285267	43.027149
3503.456600	734016.412356	43.032154
3503.387184	733974.396643	43.037159
3503.528522	733927.098731	43.042164
3503.307398	733892.631951	43.047169
3503.174323	733840.973013	43.052173
3503.616800	733801.941238	43.057178
3503.525302	733768.244617	43.062183
3503.591022	733708.532522	43.067188
3503.633954	733669.961971	43.072193
3503.484180	733624.343880	43.077197
3503.697672	733566.636060	43.082202
3503.467956	733521.030556	43.087207
3503.525777	733481.120016	43.092212
3503.627392	733432.637624	43.097217
3503.201555	733392.014247	43.102221
3503.450801	733339.546513	43.107226
3503.396656	733315.198475	43.112231
3503.237792	733252.995195	43.117236
3503.307017	733219.962890	43.122241
3503.090049	733184.749793	43.127245
3503.264502	733136.897212	43.132250
3503.225608	733105.763531	43.137255
3503.309736	733060.598783	43.142260
3502.709586	733031.092030	43.147265
3503.159210	732985.470576	43.152269
3503.185140	732948.830196	43.157274
3503.027272	732916.131117	43.162279
3503.145865	732868.038604	43.167284
3503.299815	732832.317271	43.172289
3503.145539	732797.438716	43.177293
3503.274734	732753.849125	43.182298
3503.091732	732713.528882	43.187303
3503.123373	732681.292723	43.192308
3503.010954	732634.573655	43.197313
3502.912794	732591.713795	43.202317
3503.126704	732560.140270	43.207322
3502.942766	732532.989141	43.212327
3503.296698	732481.538315	43.217332
3503.238167	732456.000136	43.222337
3503.240572	732411.587895	43.227341
3503.047186	732375.575192	43.232346
3502.862997	732344.561539	43.237351
3503.194115	732301.233309	43.242356
3503.052845	732270.806449	43.247361
3503.137372	732228.954328	43.252365
3503.011399	732191.345285	43.257370
3502.861780	732159.533016	43.262375
3503.004525	732116.630942	43.267380
3502.659545	732086.038898	43.272385
3502.842652	732059.023752	43.277389
3503.017059	732026.910002	43.282394
3503.316024	731976.801903	43.287399
3503.498687	731941.319476	43.292404
3503.435819	731912.561846	43.297409
3503.156217	731857.992982	43.302413
3503.342621	731823.697785	43.307418
3502.931482	731786.926092	43.312423
3503.460293	731752.227566	43.317428
3503.294126	731714.474380	43.322433
3503.071526	731673.759344	43.327437
3503.137015	731629.084831	43.332442
3503.102299	731597.499001	43.337447
3503.203456	731557.868920	43.342452
3503.118655	731512.723359	43.347457
3503.237791	731479.477650	43.352461
3503.463785	731435.468867	43.357466
3503.073566	731409.437341	43.362471
3503.358912	731370.172136	43.367476
3502.968663	731323.293196	43.372481
3503.077932	731282.471991	43.377485
3503.445560	731239.973887	43.382490
3503.014220	731203.450463	43.387495
3503.159957	731162.870242	43.392500
3503.127764	731129.747072	43.397505
3503.050448	731090.886907	43.402509
3502.993238	731051.924204	43.407514
3502.837809	731013.571740	43.412519
3503.310597	730970.064490	43.417524
3503.067372	730947.869858	43.422529
3503.186074	730903.529223	43.427533
3503.056035	730861.309220	43.432538
3503.153863	730832.273670	43.437543
3503.255768	730783.676308	43.442548
3502.977402	730743.560042	43.447553
3502.897828	730721.833045	43.452557
3503.339968	730685.262404	43.457562
3503.168948	730645.722233	43.462567
3502.993859	730608.757724	43.467572
3502.900582	730576.781383	43.472577
3503.045042	730543.032434	43.477581
3503.375822	730503.805076	43.482586
3502.858420	730466.450610	43.487591
3502.928736	730425.235321	43.492596
3502.506286	730390.588671	43.497601
3502.585486	730361.703079	43.502605
3503.156644	730332.042982	43.507610
3502.725687	730296.902090	43.512615
3502.965615	730257.242790	43.517620
3502.707426	730226.381788	43.522625
3503.031101	730196.613401	43.527629
3503.098653	730152.078989	43.532634
3502.764378	730125.836013	43.537639
3502.878586	730093.526427	43.542644
3502.829177	730060.698885	43.547649
3502.812522	730033.412755	43.552653
3502.985241	729994.060403	43.557658
3502.837900	729971.203452	43.562663
3502.641044	729933.595607	43.567668
3502.489112	729903.656880	43.572673
3502.554405	729874.623268	43.577677
3502.792069	729848.186101	43.582682
3502.674565	729829.087913	43.587687
3502.465102	729775.979298	43.592692
3502.552157	729762.939168	43.597697
3502.499291	729734.370275	43.602701
3502.589820	729713.454527	43.607706
3502.648420	729684.768037	43.612711
3502.912291	729647.677296	43.617716
3502.907261	729619.100116	43.622721
3502.863353	729584.140006	43.627725
3502.920061	729546.240944	43.632730
3502.691461	729522.455064	43.637735
3502.674125	729484.122149	43.642740
3502.830620	729459.232512	43.647745
3502.952505	729430.633758	43.652749
3503.285827	729384.614986	43.657754
3503.072768	729360.132649	43.662759
3503.122245	729312.624799	43.667764
3502.874840	729282.402331	43.672769
3502.961301	729240.881195	43.677773
3503.129923	729200.881780	43.682778
3502.808265	729176.416783	43.687783
3503.094330	729133.772521	43.692788
3502.907299	729102.499270	43.697793
3502.847805	729075.811370	43.702797
3502.691170	729049.733774	43.707802
3502.653891	729021.704665	43.712807
3502.834938	728989.974075	43.717812
3502.606343	728968.465073	43.722817
3502.650122	728933.834450	43.727821
3502.974420	728895.937805	43.732826
3502.829850	728865.944511	43.737831
3502.607351	728834.874210	43.742836
3502.864129	728788.617019	43.747841
3502.566580	728770.388087	43.752845
3502.632620	728734.019260	43.757850
3502.561582	728708.174137	43.762855
3502.389396	728681.503513	43.767860
3502.357084	728656.394862	43.772865
3502.160681	728629.529919	43.777869
3502.743541	728612.493006	43.782874
3502.577407	728593.300860	43.787879
3502.996653	728554.198144	43.792884
3502.552682	728519.844270	43.797889
3502.564802	728490.418202	43.802893
3502.500119	728463.431937	43.807898
3502.505543	728450.353623	43.812903
3502.639681	728420.164158	43.817908
3502.919405	728379.944267	43.822913
3502.588128	728352.753881	43.827917
3502.690067	728317.813841	43.832922
3502.563684	728293.561696	43.837927
3502.814814	728267.612557	43.842932
3502.771149	728242.405428	43.847937
3502.583979	728215.587137	43.852941
3502.568664	728183.984842	43.857946
3502.774759	728165.225731	43.862951
3502.753588	728114.750285	43.867956
3502.765666	728095.180837	43.872961
3502.397174	728065.617798	43.877965
3503.218876	728031.746857	43.882970
3502.937740	728004.646124	43.887975
3502.935143	727969.771359	43.892980
3502.841265	727938.379214	43.897985
3502.588045	727909.787396	43.902989
3502.927367	727868.713004	43.907994
3502.622345	727843.200931	43.912999
3502.770863	727799.383414	43.918004
3502.853269	727781.634600	43.923009
3502.908898	727744.718143	43.928013
3502.825947	727706.239060	43.933018
3502.623926	727695.720278	43.938023
3502.785910	727650.760315	43.943028
3502.641583	727634.435680	43.948033
3502.683299	727596.728194	43.953037
3503.172532	727556.370649	43.958042
3502.746539	727530.035327	43.963047
3502.661481	727489.524371	43.968052
3502.716170	727471.333575	43.973057
3502.842549	727438.862841	43.978061
3502.789736	727402.705838	43.983066
3502.797867	727393.687848	43.988071
3502.826244	727343.546270	43.993076
3502.749411	727323.543741	43.998081
3502.720577	727297.736741	44.003085
3502.654216	727260.887743	44.008090
3502.621973	727235.675626	44.013095
3502.658220	727196.134094	44.018100
3502.785720	727172.084504	44.023105
3502.657683	727140.546292	44.028109
3503.159459	727106.971968	44.033114
3502.839051	727078.982840	44.038119
3502.928858	727030.761447	44.043124
3502.714644	727011.623047	44.048129
3502.697166	726978.728290	44.053133
3502.839468	726949.225678	44.058138
3502.636182	726926.914401	44.063143
3502.664235	726888.363634	44.068148
3502.683961	726862.101352	44.073153
3502.716874	726827.612229	44.078157
3503.148425	726799.894610	44.083162
3502.592543	726774.172801	44.088167
3502.734124	726730.747075	44.093172
3502.768579	726718.404401	44.098177
3502.343268	726669.819842	44.103181
3502.967154	726645.786011	44.108186
3502.772081	726613.315424	44.113191
3502.685438	726591.529029	44.118196
3502.456127	726552.176786	44.123201
3502.466629	726530.423769	44.128205
3502.999793	726507.395432	44.133210
3502.990184	726475.636955	44.138215
3502.991995	726438.327091	44.143220
3502.985519	726395.617658	44.148225
3502.957910	726373.176828	44.153229
3503.171006	726327.160661	44.158234
3503.066322	726306.268358	44.163239
3503.115200	726266.522063	44.168244
3502.872759	726232.373101	44.173249
3502.662722	726194.502442	44.178253
3502.911912	726155.168548	44.183258
3502.874926	726138.773691	44.188263
3502.914657	726110.275959	44.193268
3503.073224	726071.798949	44.198273
3502.912896	726039.568114	44.203277
3502.933808	725995.514222	44.208282
3502.890805	725971.588307	44.213287
3502.785722	725935.631644	44.218292
3503.063530	725897.332373	44.223297
3502.696616	725870.932417	44.228301
3502.933563	725832.193612	44.233306
3502.745282	725806.408187	44.238311
3502.896230	725777.841424	44.243316
3502.688525	725741.008880	44.248321
3502.595411	725720.212281	44.253325
3502.940594	725685.270483	44.258330
3502.478124	725662.304729	44.263335
3502.381814	725628.723807	44.268340
3502.396833	725594.579318	44.273345
3502.554505	725572.799514	44.278349
3503.053196	725548.138917	44.283354
3502.752168	725514.293938	44.288359
3502.911370	725485.625692	44.293364
3502.762849	725453.787041	44.298369
3502.366035	725434.823704	44.303373
3502.675380	725397.706208	44.308378
3502.739532	725375.297084	44.313383
3502.848663	725339.252958	44.318388
3502.510208	725310.864321	44.323393
3502.684609	725283.976843	44.328397
3502.467815	725248.184241	44.333402
3502.662061	725219.955292	44.338407
3502.434069	725184.808479	44.343412
3502.830852	725161.451963	44.348417
3502.567180	725138.253761	44.353421
3503.028998	725104.826514	44.358426
3502.673279	725077.133698	44.363431
3502.729223	725044.962435	44.368436
3502.743479	725016.217324	44.373441
3502.582441	724980.166584	44.378445
3502.748529	724944.656470	44.383450
3502.667769	724935.501752	44.388455
3502.440457	724900.304053	44.393460
3502.729931	724880.235206	44.398465
3502.452928	724856.344599	44.403469
3502.766116	724822.544237	44.408474
3502.906819	724801.012976	44.413479
3502.810163	724754.246116	44.418484
3502.741282	724738.844885	44.423489
3502.536076	724710.630450	44.428493
3502.583844	724685.298196	44.433498
3502.378218	724648.906439	44.438503
3502.644196	724616.451100	44.443508
3502.568998	724589.404245	44.448513
3502.430690	724563.309328	44.453517
3502.664034	724531.007707	44.458522
3502.264863	724514.966644	44.463527
3502.759781	724474.146995	44.468532
3502.702028	724457.553966	44.473537
3502.289681	724426.547767	44.478541
3502.864513	724405.340422	44.483546
3502.685658	724384.207648	44.488551
3502.798365	724341.765266	44.493556
3502.681402	724316.954630	44.498561
3502.840522	724288.083985	44.503565
3502.833089	724254.334123	44.508570
3502.581275	724227.860356	44.513575
3502.494979	724194.123241	44.518580
3502.547122	724164.774176	44.523585
3502.329274	724138.740581	44.528589
3502.653588	724105.381504	44.533594
3502.716919	724093.030130	44.538599
3502.615029	724065.292081	44.543604
3502.743574	724035.087406	44.548609
3502.637481	724011.760935	44.553613
3502.681597	723974.333793	44.558618
3502.489008	723955.729890	44.563623
3502.757977	723923.965217	44.568628
3502.767381	723887.881609	44.573633
3502.652079	723861.532860	44.578637
3502.723007	723832.774282	44.583642
3502.763404	723807.837056	44.588647
3502.787704	723774.972154	44.593652
3502.575766	723744.227746	44.598657
3502.517550	723714.300491	44.603661
3502.756443	723688.933684	44.608666
3502.620824	723661.051138	44.613671
3502.464805	723629.801442	44.618676
3502.831361	723604.908992	44.623681
3502.370793	723576.782313	44.628685
3502.811019	723538.197489	44.633690
3502.539538	723514.103813	44.638695
3502.709280	723486.765152	44.643700
3502.613867	723456.396998	44.648705
3502.673575	723439.088640	44.653709
3502.821553	723394.454665	44.658714
3502.530070	723367.042905	44.663719
3502.119360	723354.124169	44.668724
3502.161413	723336.471539	44.673729
3502.451194	723307.774205	44.678733
3502.497681	723275.894998	44.683738
3502.268683	723259.575610	44.688743
3502.257110	723237.321852	44.693748
3502.474989	723218.004276	44.698753
3502.207697	723191.480160	44.703757
3502.773337	723165.264827	44.708762
3502.615292	723141.002666	44.713767
3502.544448	723107.357697	44.718772
3502.529277	723081.089093	44.723777
3502.468148	723057.207263	44.728781
3502.258073	723026.905991	44.733786
3502.383471	723015.831564	44.738791
3502.436831	722990.840167	44.743796
3502.945810	722954.174476	44.748801
3502.223007	722932.631916	44.753805
3502.580306	722906.747509	44.758810
3502.507156	722874.638621	44.763815
3502.324758	722849.735213	44.768820
3502.592365	722830.805097	44.773825
3502.577593	722808.501143	44.778829
3502.574185	722775.835111	44.783834
3502.389935	722762.878132	44.788839
3502.242949	722723.494003	44.793844
3502.785812	722702.733705	44.798849
3502.637582	722678.617281	44.803853
3502.594066	722644.371076	44.808858
3502.822639	722617.664272	44.813863
3502.828829	722585.144619	44.818868
3502.912742	722554.991460	44.823873
3502.248979	722529.521973	44.828877
3502.421705	722490.480628	44.833882
3502.602991	722477.314257	44.838887
3502.516818	722443.718685	44.843892
3502.649628	722419.456053	44.848897
3502.633448	722404.834935	44.853901
3502.677199	722374.489447	44.858906
3502.597682	722347.782965	44.863911
3502.551511	722316.906783	44.868916
3502.577816	722291.124566	44.873921
3502.640491	722264.096946	44.878925
3502.611727	722237.530465	44.883930
3502.296711	722209.870874	44.888935
3502.369838	722187.897778	44.893940
3502.379327	722155.276746	44.898945
3502.422166	722136.431654	44.903949
3502.485801	722105.338295	44.908954
3502.483732	722081.741362	44.913959
3502.479461	722046.792179	44.918964
3502.296271	722016.234899	44.923969
3502.282878	722007.512003	44.928973
3502.706573	721973.731363	44.933978
3502.438857	721966.785450	44.938983
3502.549041	721926.859406	44.943988
3502.677705	721902.348068	44.948993
3502.838238	721883.086405	44.953997
3502.450463	721848.149999	44.959002
3502.538093	721826.074404	44.964007
3502.331088	721797.652000	44.969012
3502.605135	721769.943454	44.974017
3502.511975	721754.441503	44.979021
3502.739975	721710.975095	44.984026
3502.381961	721702.110355	44.989031
3502.757460	721666.601229	44.994036
3503.086294	721639.775603	44.999041
3503.010092	721610.983968	45.004045
3502.891645	721574.713027	45.009050
3502.515745	721554.101248	45.014055
3502.547844	721527.373730	45.019060
3502.868689	721494.698796	45.024065
3502.615506	721468.018093	45.029069
3503.075208	721428.974044	45.034074
3502.865503	721402.682591	45.039079
3502.678270	721374.007585	45.044084
3502.854742	721338.430694	45.049089
3502.682963	721306.579872	45.054093
3502.703879	721270.681269	45.059098
3502.484521	721251.183261	45.064103
3502.770415	721217.273515	45.069108
3502.654141	721194.684464	45.074113
3502.614531	721170.843228	45.079117
3502.366375	721136.872410	45.084122
3502.502146	721115.629852	45.089127
3502.632775	721088.140984	45.094132
3502.841137	721060.391315	45.099137
3502.592431	721027.907553	45.104141
3502.781742	720999.317950	45.109146
3502.560648	720958.946029	45.114151
3502.310441	720946.691206	45.119156
3502.381710	720908.601176	45.124161
3502.345133	720894.526150	45.129165
3502.556591	720858.495208	45.134170
3502.300710	720837.861869	45.139175
3502.315601	720822.191626	45.144180
3502.383651	720787.671460	45.149185
3502.310647	720785.700248	45.154189
3502.442322	720754.342708	45.159194
3502.548410	720745.102975	45.164199
3502.594423	720703.495826	45.169204
3502.552779	720682.083063	45.174209
3502.286150	720662.393129	45.179213
3502.755140	720629.839137	45.184218
3502.542239	720603.496095	45.189223
3502.408148	720588.643289	45.194228
3502.737803	720555.021133	45.199233
3502.623641	720523.356144	45.204237
3502.798888	720499.427995	45.209242
3502.468944	720475.781354	45.214247
3502.551557	720440.414421	45.219252
3502.685441	720407.666856	45.224257
3502.443791	720382.121197	45.229261
3502.585026	720354.231481	45.234266
3502.507675	720339.914312	45.239271
3502.349618	720307.511964	45.244276
3502.677574	720270.913849	45.249281
3502.523582	720256.509994	45.254285
3502.498909	720215.259147	45.259290
3502.223949	720200.032174	45.264295
3502.571775	720174.785433	45.269300
3502.730130	720146.743445	45.274305
3502.620453	720131.786628	45.279309
3502.394527	720105.592912	45.284314
3502.561065	720076.904721	45.289319
3502.567551	720039.366834	45.294324
3502.508109	720029.905651	45.299329
3502.400825	719997.940010	45.304333
3502.566684	719965.383784	45.309338
3502.261853	719953.632363	45.314343
3502.394699	719929.312867	45.319348
3502.489382	719915.809602	45.324353
3502.118752	719894.399431	45.329357
3502.481670	719852.487875	45.334362
3502.148768	719841.484733	45.339367
3502.012726	719819.143138	45.344372
3502.412357	719800.928190	45.349377
3502.401341	719777.177421	45.354381
3502.731663	719747.766879	45.359386
3502.231521	719724.443671	45.364391
3502.125879	719706.311771	45.369396
3502.450393	719682.108738	45.374401
3502.379816	719655.243355	45.379405
3502.387399	719629.753496	45.384410
3502.449525	719605.841420	45.389415
3502.493970	719582.279314	45.394420
3502.473542	719552.876290	45.399425
3502.580142	719531.436140	45.404429
3502.769472	719500.857812	45.409434
3502.327463	719488.037362	45.414439
3502.292321	719461.016745	45.419444
3502.592622	719427.146929	45.424449
3502.072262	719409.975338	45.429453
3502.480911	719376.137053	45.434458
3502.156687	719362.106831	45.439463
3502.177498	719340.729917	45.444468
3502.493607	719318.163705	45.449473
3502.014177	719284.025059	45.454477
3502.388898	719266.011414	45.459482
3502.377394	719253.119666	45.464487
3502.150705	719224.493337	45.469492
3502.568267	719201.959686	45.474497
3501.877245	719177.327425	45.479501
3502.534302	719158.176012	45.484506
3502.201146	719140.377918	45.489511
3502.230897	719107.741589	45.494516
3502.265120	719108.479869	45.499521
3502.256955	719086.611159	45.504525
3502.361892	719068.343989	45.509530
3502.245864	719038.855720	45.514535
3501.903030	719015.157455	45.519540
3501.936235	718993.281683	45.524545
3501.996307	718987.171924	45.529549
3502.208784	718959.712140	45.534554
3501.974378	718949.633851	45.539559
3501.637350	718922.363674	45.544564
3502.033036	718900.328746	45.549569
3501.945579	718886.308302	45.554573
3502.553937	718876.636588	45.559578
3502.191464	718863.107759	45.564583
3502.400047	718841.549847	45.569588
3502.536544	718809.737855	45.574593
3502.579173	718794.803135	45.579597
3502.430162	718767.303095	45.584602
3502.499693	718736.741710	45.589607
3502.326762	718710.882034	45.594612
3502.062829	718683.847004	45.599617
3502.269126	718684.358591	45.604621
3502.222199	718651.038788	45.609626
3502.385461	718636.778234	45.614631
3502.594483	718618.145767	45.619636
3502.178389	718588.258994	45.624641
3502.049633	718578.708393	45.629645
3502.336573	718532.438361	45.634650
3502.318761	718520.290452	45.639655
3501.961934	718497.882504	45.644660
3502.465036	718475.332803	45.649665
3502.180493	718475.280536	45.654669
3502.341369	718445.050203	45.659674
3502.067003	718425.009076	45.664679
3502.235740	718409.308947	45.669684
3502.258939	718371.909592	45.674689
3501.871350	718351.390981	45.679693
3502.052136	718337.672591	45.684698
3501.933835	718313.588159	45.689703
3502.152558	718305.715876	45.694708
3502.353264	718285.645732	45.699713
3502.010844	718261.647675	45.704717
3502.271718	718251.933307	45.709722
3502.124456	718233.209897	45.714727
3502.109556	718214.365441	45.719732
3502.290726	718190.925673	45.724737
3502.009693	718168.256363	45.729741
3501.997710	718153.478289	45.734746
3502.222108	718142.232276	45.739751
3502.236727	718123.382751	45.744756
3502.448180	718096.168292	45.749761
3502.240041	718083.505530	45.754765
3502.338356	718038.057414	45.759770
3502.320668	718036.820410	45.764775
3502.043851	718000.907182	45.769780
3502.265630	717979.592869	45.774785
3502.037264	717966.238881	45.779789
3502.277135	717938.076849	45.784794
3502.051049	717931.715876	45.789799
3502.088592	717913.060496	45.794804
3502.511786	717874.154635	45.799809
3502.191760	717795.988927	45.804813
3502.256811	717656.006516	45.809818
3501.780936	717472.858334	45.814823
3501.731713	717232.146036	45.819828
3501.794611	716929.600872	45.824833
3501.370003	716574.442657	45.829837
3501.349241	716162.648311	45.834842
3501.108627	715681.810024	45.839847
3500.665748	715155.877340	45.844852
3500.640218	714568.514414	45.849857
3500.193836	713932.996587	45.854861
3499.789256	713230.229820	45.859866
3499.510266	712468.075011	45.864871
3499.037315	711652.823057	45.869876
3498.717280	710772.686386	45.874881
3497.714795	709851.364802	45.879885
3497.456378	708844.916235	45.884890
3496.595933	707798.175716	45.889895
3495.841262	706682.256315	45.894900
3495.089434	705511.453877	45.899905
3494.023113	704281.874202	45.904909
3493.352042	702998.543137	45.909914
3492.617051	701654.754818	45.914919
3491.754085	700261.725065	45.919924
3490.610327	698801.312227	45.924929
3489.837126	697295.500882	45.929933
3488.787925	695723.539639	45.934938
3488.036784	694099.822727	45.939943
3486.789018	692411.669320	45.944948
3485.880027	690670.449765	45.949953
3484.571991	688875.260941	45.954957
3483.307478	687017.437855	45.959962
3482.008779	685108.656281	45.964967
3480.865873	683156.423911	45.969972
3479.599590	681135.309344	45.974977
3477.984116	679078.087499	45.979981
3476.854680	676958.737233	45.984986
3475.128776	674786.019785	45.989991
3473.542130	672574.685783	45.994996
3472.432944	670301.467848	46.000001
3470.645746	667992.750872	46.005005
3468.983374	665620.292019	46.010010
3467.414016	663214.992632	46.015015
3465.810889	660751.945248	46.020020
3464.504741	658236.447837	46.025025
3462.495790	655689.504632	46.030029
3460.411903	653072.827179	46.035034
3458.613248	650421.833047	46.040039
3456.624557	647736.828438	46.045044
3455.215597	644997.066874	46.050049
3452.996155	642240.995313	46.055053
3450.828193	639411.289203	46.060058
3448.955544	636548.933530	46.065063
3446.702723	633653.268479	46.070068
3444.633754	630705.256060	46.075073
3442.419123	627741.871420	46.080077
3440.277914	624719.242445	46.085082
3438.068934	621671.221868	46.090087
3435.728007	618572.395675	46.095092
3433.675965	615440.507504	46.100097
3431.049471	612277.184517	46.105101
3428.770536	609074.431194	46.110106
3426.433335	605832.239659	46.115111
3423.726829	602563.285199	46.120116
3421.687758	599255.233700	46.125121
3418.764102	595918.361659	46.130125
3416.450099	592534.675223	46.135130
3413.712025	589130.294335	46.140135
3411.181101	585692.391280	46.145140
3408.499039	582228.297975	46.150145
3405.974128	578742.831038	46.155149
3403.331876	575215.202235	46.160154
3400.386169	571651.205337	46.165159
3397.656356	568073.689010	46.170164
3395.315523	564449.294778	46.175169
3392.280356	560815.040549	46.180173
3389.530375	557135.959071	46.185178
3386.443208	553445.286332	46.190183
3383.506164	549730.193586	46.195188
3380.668711	545970.717292	46.200193
3377.499821	542210.883172	46.205197
3374.334198	538424.821922	46.210202
3371.667734	534602.555362	46.215207
3368.729806	530754.947127	46.220212
3365.458216	526882.709308	46.225217
3362.216337	523011.027201	46.230221
3359.062207	519096.618949	46.235226
3355.866830	515180.413261	46.240231
3352.670537	511232.601336	46.245236
3349.446414	507270.821668	46.250241
3346.371579	503297.579057	46.255245
3343.210673	499297.242484	46.260250
3339.977177	495278.406357	46.265255
3336.429837	491244.200546	46.270260
3333.287419	487188.287790	46.275265
3329.748542	483130.747056	46.280269
3326.095958	479040.965927	46.285274
3322.956042	474948.514141	46.290279
3319.429464	470839.321923	46.295284
3316.043020	466711.333320	46.300289
3312.190303	462580.414551	46.305293
3308.826157	458437.807639	46.310298
3305.719309	454273.168782	46.315303
3301.776636	450116.245445	46.320308
3298.290427	445939.206658	46.325313
3294.433671	441759.138266	46.330317
3291.439224	437563.626375	46.335322
3287.730948	433354.514018	46.340327
3283.936047	429136.733829	46.345332
3280.461527	424911.248266	46.350337
3276.399852	420685.279286	46.355341
3272.740926	416455.787911	46.360346
3269.463426	412206.491669	46.365351
3265.568257	407965.884268	46.370356
3262.147050	403697.813657	46.375361
3257.983462	399440.520347	46.380365
3254.384676	395182.251392	46.385370
3250.463778	390911.634141	46.390375
3246.741940	386635.942375	46.395380
3242.955062	382353.127138	46.400385
3238.875762	378091.691708	46.405389
3235.394298	373799.264660	46.410394
3231.384922	369527.662317	46.415399
3227.587663	365250.695417	46.420404
3223.688981	360962.176065	46.425409
3219.365517	356692.342982	46.430413
3215.530226	352402.095527	46.435418
3211.637584	348125.834446	46.440423
3207.615105	343854.409179	46.445428
3203.867894	339591.743326	46.450433
3199.813989	335316.881725	46.455437
3195.990765	331027.817628	46.460442
3192.063687	326760.715677	46.465447
3187.825965	322494.633128	46.470452
3184.110839	318225.913333	46.475457
3179.577444	313983.666106	46.480461
3175.771599	309719.336808	46.485466
3171.903718	305482.135074	46.490471
3167.963309	301242.243297	46.495476
3164.028787	297008.426341	46.500481
3159.779838	292778.057126	46.505485
3155.769240	288553.329852	46.510490
3152.049866	284341.461755	46.515495
3147.617857	280129.751549	46.520500
3143.688894	275913.534813	46.525505
3139.577120	271729.336084	46.530509
3135.608494	267539.759454	46.535514
3131.699387	263347.052242	46.540519
3127.355320	259180.653390	46.545524
3123.144966	254993.243446	46.550529
3118.792813	250853.369596	46.555533
3114.775167	246704.736832	46.560538
3110.331433	242563.863885	46.565543
3106.203727	238450.662512	46.570548
3102.426289	234332.392696	46.575553
3098.040649	230243.354087	46.580557
3093.900384	226162.462642	46.585562
3089.866030	222080.004470	46.590567
3085.594619	218015.124874	46.595572
3081.764549	213967.751882	46.600577
3077.352514	209835.384270	46.605581
3073.350093	205801.897298	46.610586
3069.044069	201775.327170	46.615591
3064.729255	197780.498762	46.620596
3060.719812	193774.160117	46.625601
3056.461072	189803.535238	46.630605
3052.371878	185838.593909	46.635610
3048.204103	181869.363883	46.640615
3043.648580	177939.403262	46.645620
3039.267331	174011.537720	46.650625
3035.071299	170113.208488	46.655629
3031.112420	166219.812056	46.660634
3026.931735	162335.660350	46.665639
3022.391207	158483.694290	46.670644
3018.244155	154635.117175	46.675649
3013.831020	150806.047732	46.680653
3009.410027	147002.096843	46.685658
3005.556270	143204.512231	46.690663
3001.062338	139430.551460	46.695668
2997.088558	135660.149370	46.700673
2992.614602	131934.321000	46.705677
2988.096913	128202.831328	46.710682
2984.139665	124491.592478	46.715687
2979.388586	120804.809756	46.720692
2975.404428	117124.140154	46.725697
2970.917326	113481.963118	46.730701
2966.437986	109847.890167	46.735706
2962.292356	106245.418502	46.740711
2957.795586	102647.248819	46.745716
2953.632612	99074.827068	46.750721
2949.077793	95526.350719	46.755725
2944.491628	91994.070754	46.760730
2940.059739	88497.850848	46.765735
2935.707900	85014.030304	46.770740
2931.310333	81548.362483	46.775745
2926.556513	78127.206377	46.780749
2921.907870	74717.745004	46.785754
2917.196049	71338.617984	46.790759
2912.128139	67992.144982	46.795764
2907.471527	64664.421716	46.800769
2902.887838	61393.810190	46.805773
2897.989056	58144.426176	46.810778
2892.936901	54933.484774	46.815783
2887.545574	51757.770097	46.820788
2882.100463	48633.469638	46.825793
2875.965905	45562.228850	46.830797
2868.875421	42566.151837	46.835802
2859.376683	39704.692052	46.840807
2849.375594	36966.245564	46.845812
2839.294699	34316.873778	46.850817
2829.425850	31801.228798	46.855821
2820.298070	29412.335708	46.860826
2811.616953	27157.124543	46.865831
2802.669711	25021.516309	46.870836
2794.727911	23016.504762	46.875841
2787.107464	21137.410463	46.880845
2779.563171	19368.083354	46.885850
2772.358718	17704.152827	46.890855
2765.313632	16156.350241	46.895860
2759.069832	14692.211455	46.900865
2753.003405	13336.385751	46.905869
2747.257624	12055.199895	46.910874
2741.349819	10854.165196	46.915879
2735.700528	9722.908935	46.920884
2730.746009	8645.804297	46.925889
2725.651554	7650.991103	46.930893
2720.734797	6704.986230	46.935898
2715.774129	5814.404209	46.940903
2711.087866	4972.425202	46.945908
2706.768405	4170.204599	46.950913
2702.024196	3425.037647	46.955917
2697.255622	2719.193777	46.960922
2692.488025	2066.084342	46.965927
2686.866616	1474.461241	46.970932
2680.817383	929.724701	46.975937
2674.063824	460.137565	46.980941
2661.976560	217.768857	46.985946
2643.885736	225.508746	46.990951
2633.706555	237.089937	46.995956
2629.706430	226.986539	47.000961
2629.306989	229.731394	47.005965
2630.211720	230.777819	47.010970
2631.112702	220.977644	47.015975
2630.540015	236.907588	47.020980
2629.173182	228.382314	47.025985
2626.360252	228.265582	47.030989
2623.205257	231.289143	47.035994
2620.407585	222.452971	47.040999
2616.768654	240.262218	47.046004
2613.579583	230.811390	47.051009
2610.486563	231.829815	47.056013
2607.349865	228.762804	47.061018
2604.645555	224.446318	47.066023
2601.626902	227.674529	47.071028
2598.577928	215.085780	47.076033
2595.077327	222.386909	47.081037
2591.834612	215.762587	47.086042
2588.793626	224.372410	47.091047
2585.295955	220.942876	47.096052
2581.893561	221.288925	47.101057
2578.659833	225.780890	47.106061
2575.491862	217.824825	47.111066
2572.163821	223.589022	47.116071
2568.763682	222.496885	47.121076
2565.561430	220.633843	47.126081
2562.238899	222.850535	47.131085
2558.979166	212.484316	47.136090
2555.911688	207.912450	47.141095
2552.067342	220.278435	47.146100
2548.618507	212.907090	47.151105
2545.252873	212.185406	47.156109
2541.627537	211.982176	47.161114
2539.075645	202.061379	47.166119
2535.108423	210.834944	47.171124
2531.732115	203.321008	47.176129
2528.855073	204.764230	47.181133
2525.432586	205.339785	47.186138
2522.004168	209.730708	47.191143
2518.101769	204.988619	47.196148
2514.588225	204.344256	47.201153
2510.876550	202.367399	47.206157
2507.543803	212.771871	47.211162
2504.203034	208.043660	47.216167
2500.624890	209.290817	47.221172
2498.154508	205.325734	47.226177
2494.168492	216.096947	47.231181
2490.691028	216.209168	47.236186
2487.456074	193.415385	47.241191
2483.830126	207.402814	47.246196
2480.417732	199.348440	47.251201
2476.741984	204.691134	47.256205
2472.950632	200.177825	47.261210
2470.143549	199.742303	47.266215
2466.429441	208.768963	47.271220
2463.408856	198.913341	47.276225
2459.721331	204.705557	47.281229
2456.283861	201.460961	47.286234
2453.061330	200.177576	47.291239
2449.276116	209.598232	47.296244
2445.817274	193.357410	47.301249
2442.607630	200.106199	47.306253
2438.723638	202.920044	47.311258
2435.677880	193.745278	47.316263
2431.282288	199.542890	47.321268
2428.012012	201.136525	47.326273
2425.326639	194.852510	47.331277
2421.695683	196.699077	47.336282
2418.686241	197.765590	47.341287
2414.503082	194.379678	47.346292
2411.422959	199.334009	47.351297
2407.698323	194.494196	47.356301
2404.119376	190.101784	47.361306
2400.639750	187.429963	47.366311
2397.441573	192.540543	47.371316
2393.903755	193.556348	47.376321
2390.113329	197.860881	47.381325
2386.712502	194.448076	47.386330
2383.513342	193.557138	47.391335
2379.916158	199.608204	47.396340
2376.383343	194.108817	47.401345
2372.948833	193.950977	47.406349
2369.496002	195.422833	47.411354
2365.794705	186.588800	47.416359
2362.206049	202.488872	47.421364
2359.196040	200.436955	47.426369
2355.264636	196.201036	47.431373
2352.193242	196.523781	47.436378
2348.650936	187.502487	47.441383
2345.091161	195.828052	47.446388
2341.502584	191.731905	47.451393
2337.752715	191.541885	47.456397
2334.536189	196.784198	47.461402
2331.477011	188.579478	47.466407
2327.827524	187.105186	47.471412
2324.617121	198.217342	47.476417
2320.447447	192.143695	47.481421
2316.786560	191.437759	47.486426
2313.550804	182.832401	47.491431
2310.105442	196.735052	47.496436
2306.828184	185.648690	47.501441
2303.244903	185.888430	47.506445
2299.738673	186.395871	47.511450
2296.274613	188.883955	47.516455
2292.338783	191.618455	47.521460
2289.555638	176.399360	47.526465
2285.863603	192.091564	47.531469
2282.370911	191.308946	47.536474
2279.144443	189.191977	47.541479
2275.307054	193.299705	47.546484
2272.147834	188.854677	47.551489
2268.245948	193.750574	47.556493
2264.924115	183.249218	47.561498
2261.450728	189.846088	47.566503
2257.603317	189.466605	47.571508
2253.823518	183.586380	47.576513
2250.861603	182.120981	47.581517
2247.561347	190.312390	47.586522
2244.174640	184.111325	47.591527
2240.268853	187.716301	47.596532
2236.915221	177.824671	47.601537
2233.536023	189.776986	47.606541
2230.224370	185.896286	47.611546
2226.520180	172.688639	47.616551
2222.559498	184.411352	47.621556
2219.280982	183.994412	47.626561
2215.752233	182.840879	47.631565
2212.398752	184.226779	47.636570
2209.434937	173.820089	47.641575
2205.563100	178.478603	47.646580
2202.308756	177.429948	47.651585
2198.445419	176.548152	47.656589
2194.785540	183.156909	47.661594
2191.200471	174.930590	47.666599
2187.861953	181.321118	47.671604
2184.607841	180.714279	47.676609
2180.684671	180.893009	47.681613
2177.362791	173.316105	47.686618
2174.658268	180.524913	47.691623
2170.795216	186.952924	47.696628
2167.130073	175.883561	47.701633
2163.564920	176.530283	47.706637
2159.643888	172.809458	47.711642
2156.484144	170.231824	47.716647
2152.993533	172.313726	47.721652
2149.915457	165.651709	47.726657
2146.342343	177.527548	47.731661
2142.312556	173.864952	47.736666
2139.180543	178.542847	47.741671
2135.575584	178.962118	47.746676
2132.266847	175.772881	47.751681
2128.393904	176.495316	47.756685
2125.079512	175.197918	47.761690
2121.548208	175.370600	47.766695
2118.028000	182.434102	47.771700
2114.625853	170.549766	47.776705
2111.114225	177.583044	47.781709
2107.338166	175.114514	47.786714
2103.957831	162.889734	47.791719
2100.409973	171.416931	47.796724
2097.031223	172.337809	47.801729
2093.822557	173.735791	47.806733
2090.011766	174.886480	47.811738
2086.860699	173.607527	47.816743
2083.403838	176.720920	47.821748
2079.515082	178.666348	47.826753
2075.974139	182.576080	47.831757
2072.097840	174.691001	47.836762
2069.249800	173.757880	47.841767
2065.517687	181.549858	47.846772
2062.271066	177.083498	47.851777
2058.851617	170.265384	47.856781
2055.080047	175.680426	47.861786
2051.459785	168.212491	47.866791
2047.960197	166.207488	47.871796
2044.108974	167.898099	47.876801
2041.185804	175.632279	47.881805
2038.091371	171.867407	47.886810
2034.808194	166.925600	47.891815
2030.596999	173.319834	47.896820
2027.200313	164.146107	47.901825
2023.607531	172.379437	47.906829
2020.073449	169.453449	47.911834
2016.445229	173.023805	47.916839
2012.869993	174.981447	47.921844
2009.991318	172.248563	47.926849
2006.171358	179.710141	47.931853
2002.376617	173.999943	47.936858
1999.114528	162.686173	47.941863
1995.695031	171.142115	47.946868
1992.170451	160.262829	47.951873
1988.622409	169.123234	47.956877
1985.170390	168.692090	47.961882
1982.318887	159.488748	47.966887
1977.986687	171.110175	47.971892
1974.538683	162.434564	47.976897
1971.173987	163.758541	47.981901
1967.369174	167.899396	47.986906
1964.073208	160.581434	47.991911
1960.599733	161.103837	47.996916
1957.206125	166.675965	48.001921
1953.736699	161.017463	48.006925
1950.024565	172.746669	48.011930
1946.911444	165.477849	48.016935
1942.900819	169.579107	48.021940
1939.642936	164.867632	48.026945
1936.253403	166.907535	48.031949
1932.711956	173.641161	48.036954
1929.668069	165.119266	48.041959
1925.623638	168.770468	48.046964
1922.003999	162.597870	48.051969
1918.463321	157.267499	48.056973
1914.765108	163.120652	48.061978
1911.732541	162.390382	48.066983
1908.209479	157.060662	48.071988
1904.865969	158.331653	48.076993
1901.630246	162.143530	48.081997
1897.136556	166.881304	48.087002
1894.196522	166.582929	48.092007
1890.152971	164.183033	48.097012
1887.172152	162.918325	48.102017
1883.648545	164.460225	48.107021
1880.319700	159.677832	48.112026
1877.095134	161.668621	48.117031
1873.129080	165.578851	48.122036
1869.899198	161.473367	48.127041
1865.966517	164.005406	48.132045
1862.433397	169.707992	48.137050
1859.551280	163.225559	48.142055
1855.328751	168.665702	48.147060
1852.113267	167.603964	48.152065
1848.651183	165.634752	48.157069
1845.067285	163.974369	48.162074
1841.782399	162.908710	48.167079
1838.074960	158.284200	48.172084
1834.751855	156.887412	48.177089
1831.201026	154.933071	48.182093
1827.078973	168.568269	48.187098
1824.110635	157.248351	48.192103
1820.603075	163.059027	48.197108
1817.013918	161.031303	48.202113
1813.700520	152.283864	48.207117
1810.151610	165.653303	48.212122
1807.093322	155.760212	48.217127
1802.885526	157.914851	48.222132
1799.446187	161.189727	48.227137
1796.016783	160.932787	48.232141
1792.496694	159.330381	48.237146
1789.050104	147.343169	48.242151
1785.662564	168.661376	48.247156
1782.070165	153.018885	48.252161
1778.691274	160.357435	48.257165
1774.779569	156.581136	48.262170
1771.905842	155.798668	48.267175
1768.365781	150.612572	48.272180
1764.596138	156.296475	48.277185
1761.131542	154.945610	48.282189
1757.519342	159.449082	48.287194
1754.131732	158.805392	48.292199
1750.679463	163.338099	48.297204
1746.918670	149.529698	48.302209
1743.354389	148.905731	48.307213
1739.846253	154.891198	48.312218
1736.325215	158.807543	48.317223
1732.765457	165.901113	48.322228
1729.751129	158.677309	48.327233
1726.589869	158.624568	48.332237
1722.658552	155.346675	48.337242
1719.572648	155.807592	48.342247
1715.543626	160.305167	48.347252
1712.003780	159.880838	48.352257
1708.955746	154.730720	48.357261
1704.552930	161.158649	48.362266
1701.337057	151.410078	48.367271
1697.894710	158.309824	48.372276
1694.411945	147.961836	48.377281
1691.170059	155.744508	48.382285
1687.559462	158.204729	48.387290
1683.987377	146.691824	48.392295
1680.420302	164.867143	48.397300
1677.198783	153.213240	48.402305
1673.613476	153.859707	48.407309
1670.142465	160.717045	48.412314
1666.443875	155.467038	48.417319
1662.823573	169.142990	48.422324
1659.697310	153.723156	48.427329
1655.722995	152.962758	48.432333
1652.080376	160.019355	48.437338
1649.404392	146.141731	48.442343
1645.846008	157.172012	48.447348
1641.968460	159.315443	48.452353
1638.718074	157.770420	48.457357
1635.106742	160.140816	48.462362
1631.536131	155.537681	48.467367
1627.959996	157.575870	48.472372
1624.380333	156.180183	48.477377
1620.608453	154.125971	48.482381
1617.783503	160.225184	48.487386
1614.155740	160.030752	48.492391
1610.611401	160.457571	48.497396
1606.927824	154.168125	48.502401
1603.747557	151.510399	48.507405
1599.915332	157.635157	48.512410
1596.271396	153.914425	48.517415
1592.974688	164.034209	48.522420
1589.432197	151.044751	48.527425
1586.030292	146.418121	48.532429
1582.381888	158.395145	48.537434
1579.053520	150.499511	48.542439
1575.390151	151.354512	48.547444
1572.192171	148.570677	48.552449
1568.677257	153.242917	48.557453
1564.846102	154.880270	48.562458
1561.563173	148.894867	48.567463
1557.920371	156.351562	48.572468
1554.532266	152.705020	48.577473
1550.761399	150.876848	48.582477
1547.242264	146.378156	48.587482
1543.944345	150.577058	48.592487
1540.367630	154.642851	48.597492
1536.952104	141.840067	48.602497
1533.377820	145.250499	48.607501
1529.460844	150.594636	48.612506
1526.320517	130.210481	48.617511
1523.138360	138.565126	48.622516
1519.588222	145.361238	48.627521
1516.397616	138.258096	48.632525
1512.567260	145.922033	48.637530
1508.863832	131.209274	48.642535
1504.982418	142.041215	48.647540
1501.929420	148.037076	48.652545
1498.745908	147.978103	48.657549
1495.081442	138.500581	48.662554
1491.378433	143.916935	48.667559
1487.465997	142.956026	48.672564
1484.054813	151.432220	48.677569
1480.712511	139.527900	48.682573
1477.264608	147.008087	48.687578
1473.978597	140.133275	48.692583
1470.448830	138.549887	48.697588
1466.770243	147.193420	48.702593
1463.415770	143.344450	48.707597
1459.487627	143.745813	48.712602
1456.492975	146.581573	48.717607
1452.727764	141.863930	48.722612
1449.352196	151.207082	48.727617
1446.269094	145.774639	48.732621
1442.445762	145.210885	48.737626
1438.925554	149.085269	48.742631
1435.679014	142.974958	48.747636
1431.454535	147.829289	48.752641
1428.252201	147.333610	48.757645
1424.477384	152.671899	48.762650
1421.585705	139.024669	48.767655
1417.977184	145.758867	48.772660
1414.820899	143.891397	48.777665
1411.049812	145.696155	48.782669
1407.198663	150.330738	48.787674
1403.808526	142.299626	48.792679
1400.049410	144.431178	48.797684
1396.753749	148.277360	48.802689
1393.471959	137.397554	48.807693
1389.767437	146.578632	48.812698
1386.090078	145.310578	48.817703
1382.648185	151.016962	48.822708
1379.204126	154.630358	48.827713
1375.952925	145.787548	48.832717
1372.313740	139.190233	48.837722
1369.377084	140.793367	48.842727
1365.414389	146.430340	48.847732
1361.895207	148.297103	48.852737
1358.293606	141.046915	48.857741
1354.689644	144.004957	48.862746
1351.127360	139.139013	48.867751
1347.700253	144.383378	48.872756
1344.219827	141.255864	48.877761
1340.966015	140.390461	48.882765
1337.293270	135.255860	48.887770
1333.838535	136.887816	48.892775
1330.215454	141.633552	48.897780
1326.776449	136.135903	48.902785
1322.901436	135.244135	48.907789
1319.647407	142.294549	48.912794
1316.317472	137.058110	48.917799
1312.718050	142.462605	48.922804
1309.418412	137.785349	48.927809
1306.021943	144.889313	48.932813
1301.862987	144.484953	48.937818
1298.299819	136.515290	48.942823
1295.228099	137.566547	48.947828
1291.977049	137.970189	48.952833
1288.213092	135.859695	48.957837
1284.648483	138.211184	48.962842
1281.236766	142.258178	48.967847
1277.724005	145.912799	48.972852
1274.132434	136.654311	48.977857
1270.840308	134.869192	48.982861
1267.383786	139.383593	48.987866
1263.751606	136.782267	48.992871
1260.005787	135.765595	48.997876
1256.638889	147.913559	49.002881
1253.389931	138.245417	49.007885
1249.466857	129.246393	49.012890
1246.333335	129.243663	49.017895
1242.879337	137.165663	49.022900
1238.977638	138.680555	49.027905
1235.753556	133.878188	49.032909
1232.186405	146.091238	49.037914
1228.817477	143.287762	49.042919
1224.961986	134.372309	49.047924
1221.527076	140.139610	49.052929
1218.286964	137.905279	49.057933
1214.699710	145.235219	49.062938
1211.443438	132.125395	49.067943
1207.849552	139.016966	49.072948
1203.935340	142.959616	49.077953
1200.489755	137.527093	49.082957
1197.005100	139.604947	49.087962
1193.550492	133.331296	49.092967
1190.035768	140.322670	49.097972
1186.679777	134.484424	49.102977
1183.276396	128.899505	49.107981
1179.366375	138.406167	49.112986
1176.345291	136.035409	49.117991
1172.797110	136.259744	49.122996
1169.079285	137.373698	49.128001
1166.080865	135.582527	49.133005
1161.914095	125.908536	49.138010
1158.460323	129.854623	49.143015
1154.935513	137.981187	49.148020
1151.610144	127.995229	49.153025
1148.249465	125.938162	49.158029
1144.652015	136.703286	49.163034
1141.062421	132.862262	49.168039
1137.316238	135.501604	49.173044
1133.707911	130.202804	49.178049
1130.782138	124.552777	49.183053
1127.148976	133.691254	49.188058
1123.631244	127.131111	49.193063
1120.357758	131.864192	49.198068
1116.769265	131.038698	49.203073
1113.478061	128.808355	49.208077
1109.429156	138.226537	49.213082
1105.900542	129.073828	49.218087
1102.460910	131.490435	49.223092
1098.667509	134.650490	49.228097
1095.430935	127.073384	49.233101
1091.643724	127.271394	49.238106
1088.559130	126.224077	49.243111
1085.143430	130.902946	49.248116
1081.848338	128.542238	49.253121
1078.448471	133.537389	49.258125
1074.425057	130.776539	49.263130
1070.865468	130.880492	49.268135
1067.539232	130.385823	49.273140
1064.048663	138.382466	49.278145
1060.815103	132.501780	49.283149
1057.345254	131.564757	49.288154
1053.614405	134.542034	49.293159
1049.742368	137.824062	49.298164
1046.632549	129.819719	49.303169
1042.985027	123.713470	49.308173
1039.342045	125.222849	49.313178
1035.879410	130.062054	49.318183
1032.385125	127.763330	49.323188
1028.788262	141.756855	49.328193
1025.442050	134.243515	49.333197
1021.821163	140.342448	49.338202
1018.972511	128.540032	49.343207
1015.065048	134.428438	49.348212
1011.400134	131.560214	49.353217
1007.932014	131.882737	49.358221
1004.545498	132.535724	49.363226
1001.109323	133.019126	49.368231
997.456207	130.708608	49.373236
993.735918	135.503821	49.378241
990.414732	133.010151	49.383245
986.776464	133.921260	49.388250
983.353729	131.109312	49.393255
980.028800	129.283068	49.398260
976.464920	132.181290	49.403265
973.014376	125.546622	49.408269
969.360365	133.826104	49.413274
965.741658	135.311795	49.418279
962.458951	140.046905	49.423284
958.723192	132.859709	49.428289
955.872969	129.159815	49.433293
952.036883	133.576776	49.438298
948.366537	127.273100	49.443303
944.782486	128.617703	49.448308
940.888715	123.636035	49.453313
938.015346	121.557347	49.458317
934.510748	131.317025	49.463322
930.980054	122.425301	49.468327
927.502906	119.873608	49.473332
924.256797	124.836135	49.478337
920.648415	117.862547	49.483341
916.429560	136.861414	49.488346
913.368076	127.515193	49.493351
909.815155	127.091284	49.498356
906.004157	131.625691	49.503361
903.170868	125.722741	49.508365
899.367655	132.328284	49.513370
896.351568	123.370624	49.518375
892.603898	122.952298	49.523380
888.710639	126.974621	49.528385
885.169013	118.863040	49.533389
881.669649	134.165833	49.538394
878.373237	123.187459	49.543399
874.617289	128.669074	49.548404
871.545977	131.947675	49.553409
868.046857	126.099619	49.558413
864.174008	131.485728	49.563418
860.895612	127.262342	49.568423
857.463506	132.408219	49.573428
854.092096	126.758489	49.578433
850.430420	122.297964	49.583437
846.388871	128.335372	49.588442
843.351196	127.465961	49.593447
839.498822	128.978560	49.598452
836.255458	117.799641	49.603457
832.848769	127.218378	49.608461
829.207256	129.635820	49.613466
825.643831	132.622095	49.618471
822.463339	128.004056	49.623476
818.774643	126.967258	49.628481
815.449008	128.199166	49.633485
811.735523	121.773298	49.638490
808.455509	121.327813	49.643495
804.851972	121.215468	49.648500
800.984508	118.953598	49.653505
797.918127	117.837957	49.658509
794.237507	126.851119	49.663514
791.031583	116.220757	49.668519
787.367178	114.523632	49.673524
783.596392	125.541841	49.678529
780.151072	111.122588	49.683533
776.431270	126.959386	49.688538
773.252686	122.732781	49.693543
769.738111	122.420649	49.698548
766.205240	128.598746	49.703553
763.107197	124.718174	49.708557
759.163752	128.115065	49.713562
755.784859	123.999555	49.718567
752.379018	130.813383	49.723572
748.682659	124.054398	49.728577
745.200719	129.589851	49.733581
741.507511	127.110949	49.738586
738.120431	125.811598	49.743591
734.867584	129.929788	49.748596
731.209604	118.198926	49.753601
728.125804	120.306923	49.758605
724.082743	120.560592	49.763610
720.682117	118.004104	49.768615
717.270924	119.848360	49.773620
713.639377	122.681017	49.778625
710.212308	119.436659	49.783629
706.203385	119.599843	49.788634
703.282486	125.600576	49.793639
699.820791	121.400538	49.798644
696.181244	116.537280	49.803649
692.696817	119.408367	49.808653
688.855231	121.793701	49.813658
685.928816	115.264383	49.818663
682.170260	120.045842	49.823668
678.332847	123.837888	49.828673
675.299783	115.116069	49.833677
671.641204	117.738530	49.838682
668.042137	128.281256	49.843687
664.541318	124.130540	49.848692
661.042909	123.170535	49.853697
657.801379	112.159599	49.858701
654.452575	115.941277	49.863706
650.858771	123.539299	49.868711
647.182936	108.030147	49.873716
643.225395	129.380832	49.878721
639.870463	116.579108	49.883725
636.719487	121.113463	49.888730
632.917373	119.434121	49.893735
629.593921	119.839169	49.898740
626.889514	116.711725	49.903745
623.128613	114.634653	49.908749
618.757593	118.695989	49.913754
615.551163	121.746300	49.918759
612.064798	125.351658	49.923764
608.448305	119.763009	49.928769
605.249138	109.051573	49.933773
601.462207	129.493156	49.938778
598.201190	117.317269	49.943783
594.410476	118.236948	49.948788
590.934620	131.246554	49.953793
587.454741	114.555162	49.958797
583.694631	123.954395	49.963802
580.752461	123.788060	49.968807
577.234750	121.936600	49.973812
573.618609	116.594000	49.978817
570.076338	121.401923	49.983821
566.586029	120.508932	49.988826
563.229151	119.157164	49.993831
559.525650	122.746788	49.998836
556.093270	127.829386	50.003841
552.513988	120.833156	50.008845
548.998409	118.382061	50.013850
545.593648	115.905134	50.018855
541.698479	121.243299	50.023860
538.302517	125.041154	50.028865
535.379536	113.152952	50.033869
531.456176	126.624008	50.038874
528.083013	120.055260	50.043879
525.007273	115.092546	50.048884
521.034268	129.155542	50.053889
517.596876	116.393819	50.058893
514.120156	124.711785	50.063898
510.706588	119.158513	50.068903
506.651908	120.974433	50.073908
503.205334	126.082308	50.078913
500.003711	116.438747	50.083917
496.341086	122.460911	50.088922
493.185628	117.073330	50.093927
489.704098	122.048470	50.098932
485.496274	119.894908	50.103937
482.320993	114.246977	50.108941
478.977315	125.008450	50.113946
475.550985	110.691719	50.118951
472.228135	120.206539	50.123956
468.491215	127.089955	50.128961
465.088155	110.827216	50.133965
461.268552	124.060138	50.138970
457.794301	114.658076	50.143975
454.293404	126.517702	50.148980
450.698924	119.963346	50.153985
447.527913	110.578405	50.158989
443.702359	122.527282	50.163994
440.331282	119.084636	50.168999
436.942413	117.875804	50.174004
433.766600	116.793727	50.179009
429.966428	117.008064	50.184013
426.544189	115.747930	50.189018
423.140680	117.758874	50.194023
419.546007	123.371829	50.199028
415.622709	120.232727	50.204033
412.566950	122.461803	50.209037
408.907564	115.019370	50.214042
405.555767	112.376517	50.219047
401.608701	119.316862	50.224052
398.216314	118.671244	50.229057
395.223563	103.871199	50.234061
391.242039	123.356275	50.239066
387.809300	115.799587	50.244071
384.125622	117.145933	50.249076
381.042369	118.976624	50.254081
377.668849	114.371543	50.259085
373.926190	117.369481	50.264090
370.127418	120.827420	50.269095
366.690517	114.934772	50.274100
363.162590	119.808757	50.279105
359.921193	114.514438	50.284109
356.142904	119.421183	50.289114
353.045180	120.089030	50.294119
349.379669	117.927937	50.299124
345.694396	118.139512	50.304129
342.453820	110.983027	50.309133
338.862170	117.771852	50.314138
335.558456	115.567663	50.319143
331.836681	109.758507	50.324148
327.915861	115.185950	50.329153
324.876173	110.471985	50.334157
321.654943	111.407556	50.339162
317.754795	116.270959	50.344167
314.508403	113.286709	50.349172
310.842099	111.175906	50.354177
306.746180	112.681127	50.359181
303.435306	121.305088	50.364186
300.562812	117.385164	50.369191
297.123279	126.555731	50.374196
293.258273	122.060486	50.379201
289.912252	119.851496	50.384205
285.961436	126.900110	50.389210
282.933688	122.023763	50.394215
279.605123	118.789701	50.399220
275.662351	125.050614	50.404225
272.395627	117.604879	50.409229
268.597491	126.067392	50.414234
265.120423	118.851841	50.419239
261.796496	121.274398	50.424244
257.782474	105.253895	50.429249
254.839463	119.437264	50.434253
251.073769	128.285538	50.439258
247.688013	117.146881	50.444263
244.188160	117.585568	50.449268
240.981250	120.880523	50.454273
237.381460	114.752497	50.459277
234.092580	117.196110	50.464282
230.291446	115.335223	50.469287
226.632828	114.392424	50.474292
223.184345	118.741876	50.479297
220.094301	115.257822	50.484301
216.023512	119.723715	50.489306
212.538325	127.073008	50.494311
209.383827	113.587889	50.499316
205.505168	125.593298	50.504321
202.288091	111.329407	50.509325
198.482432	125.234903	50.514330
195.558806	112.710876	50.519335
191.917552	123.208829	50.524340
188.345753	121.655347	50.529345
184.770464	116.388226	50.534349
180.853812	118.368274	50.539354
177.682462	113.398173	50.544359
174.211694	112.878782	50.549364
170.615854	123.851121	50.554369
167.457335	116.837088	50.559373
163.649996	119.595494	50.564378
159.887253	113.269358	50.569383
156.523274	124.644561	50.574388
153.128706	113.562113	50.579393
149.762871	116.282168	50.584397
145.849248	122.247891	50.589402
142.958248	115.538869	50.594407
139.620858	112.871745	50.599412
135.763574	110.240969	50.604417
132.292828	112.901445	50.609421
128.419289	118.527446	50.614426
124.698111	126.173395	50.619431
121.635453	117.952420	50.624436
118.029981	115.469015	50.629441
114.884694	103.156402	50.634445
111.278503	114.446226	50.639450
107.852286	125.517611	50.644455
104.367003	113.348711	50.649460
100.513889	117.760316	50.654465
97.000877	117.787493	50.659469
93.525479	110.157422	50.664474
89.910852	123.088507	50.669479
86.593463	100.648043	50.674484
83.017437	109.652306	50.679489
79.350523	104.984563	50.684493
76.082622	118.778214	50.689498
72.583487	115.805220	50.694503
68.939665	112.605178	50.699508
65.667831	117.641032	50.704513
62.256922	112.024363	50.709517
58.571314	117.826506	50.714522
54.749140	114.642588	50.719527
51.295374	120.929087	50.724532
48.047271	116.089211	50.729537
44.768165	112.943451	50.734541
41.230576	116.489453	50.739546
37.953295	108.222393	50.744551
34.322568	119.542584	50.749556
30.215242	119.164827	50.754561
27.020622	114.101020	50.759565
23.540876	115.877242	50.764570
19.921559	109.736469	50.769575
16.473497	117.402198	50.774580
12.998981	111.901480	50.779585
9.339711	111.049359	50.784589
5.528655	113.471866	50.789594
2.617126	118.496647	50.794599