Thu Mar 11 19:49:48 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.405561	0.177509	0.000000	0.000094	0.719613

0.751683	0.110742	0.005005	0.000029	0.719603
0.647601	0.130487	0.010010	0.000049	0.719605
0.392681	0.177136	0.015014	0.000096	0.719608
0.278489	0.195277	0.020019	0.000118	0.719603
0.568748	0.146852	0.025024	0.000064	0.719609
0.299284	0.191498	0.030029	0.000114	0.719603
0.414813	0.065414	0.035034	0.000093	0.719394
0.612885	-0.030231	0.040038	0.000056	0.719275
0.512604	-0.015674	0.045043	0.000075	0.719268
0.368654	0.014575	0.050048	0.000102	0.719277
0.365909	0.011524	0.055053	0.000102	0.719270
0.351653	0.015192	0.060058	0.000105	0.719272
0.500927	-0.009314	0.065062	0.000078	0.719276
0.630774	-0.036454	0.070067	0.000053	0.719268
0.724094	-0.046682	0.075072	0.000036	0.719280
0.322107	0.020026	0.080077	0.000111	0.719270
0.222473	0.039850	0.085082	0.000130	0.719274
0.355270	0.017407	0.090086	0.000105	0.719277
0.173018	0.036750	0.095091	0.000139	0.719250
0.179589	-0.106545	0.100096	0.000138	0.718970
0.476057	-0.164388	0.105101	0.000083	0.718960
0.548934	-0.176001	0.110106	0.000070	0.718962
0.274006	-0.126144	0.115110	0.000121	0.718964
0.177091	-0.111354	0.120115	0.000139	0.718959
0.547818	-0.172692	0.125120	0.000070	0.718968
0.400182	-0.233544	0.130125	0.000098	0.718796
0.276059	-0.285910	0.135130	0.000121	0.718648
0.480413	-0.321257	0.140134	0.000083	0.718650
0.441528	-0.318857	0.145139	0.000090	0.718641
0.490933	-0.322337	0.150144	0.000081	0.718651
0.542260	-0.425147	0.155149	0.000072	0.718466
0.527109	-0.478354	0.160154	0.000075	0.718356
0.376654	-0.450586	0.165158	0.000103	0.718357
0.328161	-0.446314	0.170163	0.000112	0.718349
0.477908	-0.551799	0.175168	0.000084	0.718193
0.298238	-0.609575	0.180173	0.000118	0.718015
0.342022	-0.615811	0.185178	0.000110	0.718018
0.653466	-0.670037	0.190182	0.000052	0.718020
0.360371	-0.750515	0.195187	0.000107	0.717758
0.038266	-0.716536	0.200192	0.000167	0.717711
-0.181318	-0.681509	0.205197	0.000208	0.717703
0.147192	-0.781102	0.210202	0.000147	0.717622
0.273428	-0.923447	0.215206	0.000124	0.717385
-0.042941	-0.872085	0.220211	0.000183	0.717375
0.272018	-0.929546	0.225216	0.000124	0.717372
0.414382	-1.100090	0.230221	0.000098	0.717084
0.477079	-1.109185	0.235226	0.000086	0.717088
0.303929	-1.111063	0.240230	0.000119	0.717023
0.316549	-1.249594	0.245235	0.000116	0.716753
0.375287	-1.255264	0.250240	0.000106	0.716763
-0.020604	-1.261687	0.255245	0.000179	0.716610
-0.007363	-1.345741	0.260250	0.000177	0.716448
0.152633	-1.369450	0.265254	0.000147	0.716457
0.161070	-1.506891	0.270259	0.000146	0.716188
0.217755	-1.541592	0.275264	0.000136	0.716139
-0.102754	-1.528323	0.280269	0.000195	0.716052
-0.324574	-1.573157	0.285274	0.000237	0.715885
-0.090249	-1.613066	0.290278	0.000193	0.715888
-0.053608	-1.763847	0.295283	0.000187	0.715602
0.001202	-1.798076	0.300288	0.000177	0.715553
-0.089520	-1.863844	0.305293	0.000194	0.715391
0.012398	-1.959582	0.310298	0.000175	0.715237
-0.104160	-1.983099	0.315302	0.000197	0.715149
-0.263867	-2.075744	0.320307	0.000227	0.714908
-0.535871	-2.029428	0.325312	0.000277	0.714904
-1.812222	-1.950811	0.330317	0.000515	0.714608
-1.828212	-1.946918	0.335322	0.000518	0.714610
-2.090137	-1.952751	0.340326	0.000567	0.714506
-3.333940	-1.846362	0.345331	0.000799	0.714277
-2.754099	-1.946933	0.350336	0.000691	0.714282
-3.230398	-1.895844	0.355341	0.000780	0.714215
-4.267299	-1.832587	0.360346	0.000973	0.713973
-3.827062	-1.909702	0.365350	0.000891	0.713975
-4.286750	-1.832730	0.370355	0.000977	0.713965
-4.049985	-1.971965	0.375360	0.000933	0.713772
-5.268985	-1.815023	0.380365	0.001160	0.713652
-5.214616	-1.823039	0.385370	0.001150	0.713655
-5.068205	-1.848278	0.390374	0.001123	0.713657
-5.084639	-1.929799	0.395379	0.001126	0.713489
-5.672477	-1.885517	0.400384	0.001235	0.713368
-5.760027	-1.872486	0.405389	0.001252	0.713363
-6.233631	-1.788592	0.410394	0.001340	0.713362
-5.820709	-1.899534	0.415398	0.001263	0.713287
-6.779391	-1.861605	0.420403	0.001442	0.713023
-7.001979	-1.817139	0.425408	0.001483	0.713032
-7.235807	-1.779533	0.430413	0.001527	0.713024
-6.859252	-1.844525	0.435418	0.001457	0.713028
-6.630273	-1.914872	0.440422	0.001414	0.712969
-8.164153	-1.771136	0.445427	0.001700	0.712711
-7.567022	-1.873511	0.450432	0.001589	0.712719
-8.039163	-1.792108	0.455437	0.001677	0.712713
-7.790306	-1.834310	0.460442	0.001631	0.712717
-7.565533	-1.873435	0.465446	0.001589	0.712719
-7.934763	-1.922548	0.470451	0.001658	0.712490
-8.663579	-1.840120	0.475456	0.001794	0.712395
-8.538497	-1.864540	0.480461	0.001771	0.712390
-8.739969	-1.829246	0.485466	0.001808	0.712389
-8.596345	-1.853561	0.490470	0.001782	0.712391
-8.903207	-1.802270	0.495475	0.001839	0.712384
-9.030760	-1.910290	0.500480	0.001863	0.712124
-9.424535	-1.857258	0.505485	0.001936	0.712089
-9.981072	-1.756854	0.510490	0.002040	0.712092
-9.488579	-1.842472	0.515494	0.001948	0.712096
-9.550558	-1.834500	0.520499	0.001960	0.712089
-9.370408	-1.862230	0.525504	0.001926	0.712098
-10.004292	-1.889213	0.530509	0.002045	0.711819
-10.612927	-1.809551	0.535514	0.002158	0.711761
-10.069171	-1.904425	0.540518	0.002057	0.711765
-10.432914	-1.842601	0.545523	0.002125	0.711759
-10.691532	-1.791406	0.550528	0.002173	0.711769
-10.233430	-1.876223	0.555533	0.002088	0.711762
-10.413975	-1.923804	0.560538	0.002122	0.711603
-11.637651	-1.776994	0.565542	0.002349	0.711461
-11.433503	-1.817185	0.570547	0.002311	0.711453
-11.128281	-1.867599	0.575552	0.002255	0.711461
-11.554250	-1.794958	0.580557	0.002334	0.711454
-11.450134	-1.813215	0.585562	0.002315	0.711454
-11.266284	-1.843762	0.590566	0.002281	0.711459
-11.973898	-1.831965	0.595571	0.002413	0.711230
-12.298163	-1.816911	0.600576	0.002473	0.711145
-12.079761	-1.859211	0.605581	0.002433	0.711138
-12.523394	-1.779234	0.610586	0.002515	0.711140
-12.585305	-1.765402	0.615590	0.002527	0.711145
-12.463428	-1.791713	0.620595	0.002504	0.711136
-12.291121	-1.817741	0.625600	0.002472	0.711145
-12.549135	-1.837873	0.630605	0.002521	0.711013
-13.168162	-1.798194	0.635610	0.002636	0.710871
-12.669213	-1.883292	0.640614	0.002543	0.710879
-13.315838	-1.771246	0.645619	0.002664	0.710872
-13.153266	-1.797497	0.650624	0.002633	0.710878
-12.959404	-1.834445	0.655629	0.002597	0.710873
-13.115322	-1.807341	0.660634	0.002627	0.710871
-13.303806	-1.919098	0.665638	0.002662	0.710581
-14.053785	-1.809498	0.670643	0.002801	0.710532
-14.222283	-1.774251	0.675648	0.002833	0.710543
-14.007469	-1.816222	0.680653	0.002793	0.710535
-14.018018	-1.815335	0.685658	0.002795	0.710533
-13.752055	-1.859895	0.690662	0.002746	0.710538
-14.059875	-1.821312	0.695667	0.002803	0.710506
-14.702039	-1.845930	0.700672	0.002923	0.710228
-14.731821	-1.843412	0.705677	0.002929	0.710222
-15.315050	-1.741445	0.710682	0.003037	0.710218
-15.252645	-1.749419	0.715686	0.003026	0.710224
-14.800814	-1.834721	0.720691	0.002942	0.710214
-14.605780	-1.865159	0.725696	0.002905	0.710222
-14.972014	-1.803581	0.730701	0.002974	0.710215
-15.642566	-1.843691	0.735706	0.003099	0.709896
-15.595361	-1.851261	0.740710	0.003090	0.709897
-15.985038	-1.785345	0.745715	0.003163	0.709890
-15.972362	-1.782663	0.750720	0.003160	0.709900
-15.901548	-1.799086	0.755725	0.003147	0.709892
-16.155262	-1.753731	0.760730	0.003195	0.709892
-15.836059	-1.808291	0.765734	0.003135	0.709896
-16.196929	-1.843025	0.770739	0.003203	0.709698
-16.891879	-1.766762	0.775744	0.003332	0.709603
-16.665676	-1.812282	0.780749	0.003290	0.709592
-17.017650	-1.749258	0.785754	0.003356	0.709592
-16.693996	-1.803951	0.790758	0.003296	0.709598
-16.982662	-1.755800	0.795763	0.003349	0.709591
-17.087800	-1.732552	0.800768	0.003369	0.709600
-16.755601	-1.829661	0.805773	0.003307	0.709524
-17.720220	-1.788177	0.810778	0.003487	0.709263
-17.913942	-1.749729	0.815782	0.003523	0.709271
-18.226058	-1.698292	0.820787	0.003581	0.709262
-17.434553	-1.834653	0.825792	0.003434	0.709271
-17.599846	-1.809384	0.830797	0.003465	0.709263
-18.117479	-1.717381	0.835802	0.003562	0.709262
-17.412038	-1.840001	0.840806	0.003430	0.709268
-18.069245	-1.856606	0.845811	0.003553	0.709000
-18.823878	-1.742050	0.850816	0.003693	0.708960
-18.810248	-1.747303	0.855821	0.003691	0.708954
-18.324002	-1.834409	0.860826	0.003601	0.708953
-18.576033	-1.786973	0.865830	0.003648	0.708958
-19.021880	-1.711583	0.870835	0.003731	0.708950
-18.482372	-1.801632	0.875840	0.003630	0.708962
-18.894058	-1.825999	0.880845	0.003707	0.708766
-19.919131	-1.705360	0.885850	0.003898	0.708641
-18.986991	-1.871433	0.890854	0.003725	0.708641
-19.473519	-1.788905	0.895859	0.003815	0.708633
-20.079733	-1.675888	0.900864	0.003928	0.708642
-19.379554	-1.804399	0.905869	0.003798	0.708635
-19.460719	-1.787143	0.910874	0.003813	0.708640
-19.727574	-1.804745	0.915878	0.003863	0.708509
-20.611507	-1.729295	0.920883	0.004028	0.708345
-19.862169	-1.857882	0.925888	0.003888	0.708354
-20.403949	-1.763244	0.930893	0.003989	0.708350
-21.006335	-1.655856	0.935898	0.004102	0.708350
-20.302008	-1.778212	0.940902	0.003971	0.708356
-20.160380	-1.806899	0.945907	0.003944	0.708349
-20.254425	-1.862672	0.950912	0.003962	0.708204
-21.522467	-1.732812	0.955917	0.004198	0.708011
-21.321299	-1.769151	0.960922	0.004161	0.708010
-21.270711	-1.774018	0.965926	0.004151	0.708018
-21.428707	-1.751947	0.970931	0.004181	0.708005
-21.124425	-1.801526	0.975936	0.004124	0.708014
-21.286645	-1.773874	0.980941	0.004155	0.708012
-21.412170	-1.787721	0.985946	0.004178	0.707939
-21.838770	-1.829512	0.990950	0.004258	0.707702
-22.160081	-1.776226	0.995955	0.004318	0.707694
-22.647947	-1.683837	1.000960	0.004409	0.707705
-22.264351	-1.753470	1.005965	0.004337	0.707702
-21.902283	-1.819656	1.010970	0.004270	0.707699
-22.110488	-1.780694	1.015974	0.004309	0.707702
-22.336966	-1.765285	1.020979	0.004351	0.707652
-22.630361	-1.849126	1.025984	0.004406	0.707379
-22.782931	-1.822958	1.030989	0.004434	0.707376
-23.544310	-1.687806	1.035994	0.004576	0.707375
-22.768330	-1.822753	1.040998	0.004432	0.707381
-22.621687	-1.854236	1.046003	0.004405	0.707371
-22.899838	-1.800667	1.051008	0.004457	0.707378
-23.131682	-1.824889	1.056013	0.004500	0.707247
-24.141544	-1.726747	1.061018	0.004688	0.707082
-23.786624	-1.788394	1.066022	0.004622	0.707085
-23.909249	-1.771684	1.071027	0.004645	0.707075
-23.965953	-1.758793	1.076032	0.004656	0.707080
-23.617051	-1.822750	1.081037	0.004591	0.707076
-23.929356	-1.765854	1.086042	0.004649	0.707078
-23.793450	-1.862128	1.091046	0.004624	0.706934
-24.961695	-1.747952	1.096051	0.004841	0.706745
-24.795748	-1.771875	1.101056	0.004811	0.706756
-24.912122	-1.754061	1.106061	0.004832	0.706750
-24.771801	-1.778818	1.111066	0.004806	0.706750
-24.393815	-1.842908	1.116070	0.004736	0.706756
-25.021511	-1.733639	1.121075	0.004853	0.706751
-24.847464	-1.823623	1.126080	0.004821	0.706632
-25.497051	-1.801816	1.131085	0.004942	0.706443
-25.878406	-1.735173	1.136090	0.005013	0.706440
-25.813462	-1.743386	1.141094	0.005001	0.706447
-25.584934	-1.788800	1.146099	0.004959	0.706437
-25.380065	-1.820441	1.151104	0.004921	0.706447
-25.942438	-1.721996	1.156109	0.005025	0.706443
-25.796255	-1.788618	1.161114	0.004998	0.706361
-26.348174	-1.804486	1.166118	0.005101	0.706131
-26.514429	-1.778747	1.171123	0.005132	0.706123
-26.660469	-1.749119	1.176128	0.005159	0.706130
-26.312638	-1.811760	1.181133	0.005095	0.706129
-26.529527	-1.775093	1.186138	0.005135	0.706125
-26.687743	-1.742480	1.191142	0.005165	0.706133
-26.507957	-1.817829	1.196147	0.005132	0.706046
-27.288449	-1.767400	1.201152	0.005277	0.705868
-27.302902	-1.767517	1.206157	0.005280	0.705862
-27.398723	-1.750956	1.211162	0.005298	0.705861
-27.285795	-1.766251	1.216166	0.005277	0.705870
-27.604717	-1.712597	1.221171	0.005336	0.705864
-27.244558	-1.774022	1.226176	0.005269	0.705869
-27.067467	-1.886977	1.231181	0.005236	0.705705
-28.442155	-1.730303	1.236186	0.005492	0.705527
-28.359040	-1.743041	1.241190	0.005477	0.705531
-28.085881	-1.794739	1.246195	0.005426	0.705525
-27.963197	-1.812242	1.251200	0.005404	0.705533
-28.218032	-1.768574	1.256205	0.005451	0.705530
-28.654739	-1.692019	1.261210	0.005533	0.705527
-28.254612	-1.843181	1.266214	0.005458	0.705366
-29.336553	-1.727053	1.271219	0.005660	0.705211
-29.139705	-1.757392	1.276224	0.005623	0.705221
-29.103718	-1.767351	1.281229	0.005617	0.705213
-29.367676	-1.720931	1.286234	0.005666	0.705212
-29.252935	-1.737175	1.291238	0.005645	0.705220
-29.179486	-1.754937	1.296243	0.005631	0.705210
-28.972046	-1.864503	1.301248	0.005593	0.705064
-30.204722	-1.730571	1.306253	0.005822	0.704891
-29.978254	-1.772084	1.311258	0.005780	0.704889
-29.678304	-1.822706	1.316262	0.005724	0.704894
-30.346634	-1.706946	1.321267	0.005849	0.704887
-30.126434	-1.742924	1.326272	0.005808	0.704893
-29.775384	-1.807732	1.331277	0.005743	0.704889
-30.055854	-1.844306	1.336282	0.005795	0.704714
-31.378174	-1.663820	1.341286	0.006041	0.704603
-30.979440	-1.740654	1.346291	0.005967	0.704591
-30.624858	-1.801251	1.351296	0.005901	0.704596
-31.027032	-1.730535	1.356301	0.005976	0.704594
-31.165546	-1.707561	1.361306	0.006002	0.704590
-30.702639	-1.788089	1.366310	0.005916	0.704594
-30.933775	-1.809835	1.371315	0.005959	0.704467
-32.101053	-1.702033	1.376320	0.006177	0.704264
-31.530239	-1.805054	1.381325	0.006071	0.704262
-31.934212	-1.734093	1.386330	0.006146	0.704259
-31.776620	-1.759572	1.391334	0.006117	0.704264
-31.725614	-1.773443	1.396339	0.006107	0.704255
-31.760050	-1.761163	1.401344	0.006114	0.704267
-31.800227	-1.805232	1.406349	0.006121	0.704163
-32.990704	-1.699475	1.411354	0.006343	0.703948
-32.304599	-1.817596	1.416358	0.006215	0.703957
-32.886332	-1.718501	1.421363	0.006324	0.703947
-32.954292	-1.702607	1.426368	0.006337	0.703955
-32.401813	-1.801703	1.431373	0.006234	0.703953
-32.238818	-1.831011	1.436378	0.006204	0.703952
-32.723000	-1.816208	1.441382	0.006294	0.703808
-33.923719	-1.690152	1.446387	0.006518	0.703630
-33.312992	-1.793098	1.451392	0.006404	0.703642
-33.459858	-1.769791	1.456397	0.006431	0.703636
-33.965646	-1.679358	1.461402	0.006526	0.703636
-33.227586	-1.808294	1.466406	0.006388	0.703641
-33.149030	-1.825603	1.471411	0.006374	0.703635
-33.805867	-1.783268	1.476416	0.006496	0.703483
-34.475033	-1.732917	1.481421	0.006621	0.703344
-34.113807	-1.799850	1.486426	0.006554	0.703339
-34.339804	-1.755280	1.491430	0.006596	0.703347
-34.486507	-1.733623	1.496435	0.006623	0.703338
-34.276202	-1.766264	1.501440	0.006584	0.703347
-34.290572	-1.767389	1.506445	0.006587	0.703340
-34.680201	-1.795814	1.511450	0.006660	0.703142
-35.224758	-1.763005	1.516454	0.006761	0.703012
-35.160061	-1.779464	1.521459	0.006749	0.703002
-35.402865	-1.732709	1.526464	0.006795	0.703009
-35.386981	-1.737373	1.531469	0.006792	0.703005
-34.936909	-1.817713	1.536474	0.006708	0.703004
-35.317528	-1.745188	1.541478	0.006779	0.703013
-35.948312	-1.725001	1.546483	0.006897	0.702827
-36.062600	-1.767372	1.551488	0.006918	0.702700
-35.728766	-1.829112	1.556493	0.006856	0.702695
-36.331202	-1.722136	1.561498	0.006968	0.702694
-36.175004	-1.746255	1.566502	0.006939	0.702701
-36.057886	-1.773178	1.571507	0.006918	0.702689
-36.151000	-1.751570	1.576512	0.006935	0.702699
-36.440871	-1.792549	1.581517	0.006989	0.702511
-37.197180	-1.728714	1.586522	0.007130	0.702368
-36.533709	-1.842629	1.591526	0.007007	0.702376
-37.161238	-1.734689	1.596531	0.007124	0.702368
-37.100778	-1.740775	1.601536	0.007112	0.702377
-37.022805	-1.756276	1.606541	0.007098	0.702374
-37.517212	-1.670104	1.611546	0.007190	0.702370
-37.055171	-1.812184	1.616550	0.007104	0.702249
-37.860927	-1.755517	1.621555	0.007254	0.702073
-37.704476	-1.780650	1.626560	0.007225	0.702078
-37.940274	-1.738967	1.631565	0.007269	0.702077
-37.789920	-1.767181	1.636570	0.007241	0.702074
-37.501608	-1.816059	1.641574	0.007188	0.702079
-38.388013	-1.661723	1.646579	0.007353	0.702071
-38.108609	-1.806050	1.651584	0.007301	0.701880
-38.652357	-1.773333	1.656589	0.007402	0.701750
-38.671332	-1.772549	1.661594	0.007406	0.701744
-38.712982	-1.760663	1.666598	0.007414	0.701753
-38.862059	-1.738878	1.671603	0.007442	0.701743
-38.677183	-1.767732	1.676608	0.007407	0.701751
-38.678731	-1.768397	1.681613	0.007408	0.701749
-39.224217	-1.788493	1.686618	0.007510	0.701511
-39.529550	-1.766139	1.691622	0.007567	0.701446
-39.850807	-1.713301	1.696627	0.007626	0.701437
-39.579067	-1.758843	1.701632	0.007576	0.701443
-39.600873	-1.755933	1.706637	0.007580	0.701441
-39.759808	-1.728416	1.711642	0.007610	0.701439
-39.480592	-1.774751	1.716646	0.007558	0.701446
-39.659507	-1.860351	1.721651	0.007591	0.701207
-40.413741	-1.765371	1.726656	0.007732	0.701127
-40.686748	-1.716047	1.731661	0.007783	0.701128
-40.584295	-1.737299	1.736666	0.007764	0.701122
-40.300928	-1.783452	1.741670	0.007711	0.701131
-40.382770	-1.772302	1.746675	0.007727	0.701124
-40.347230	-1.776034	1.751680	0.007720	0.701129
-40.666530	-1.840743	1.756685	0.007780	0.700882
-41.009888	-1.783419	1.761690	0.007844	0.700874
-41.345624	-1.718017	1.766694	0.007906	0.700885
-41.200038	-1.748076	1.771699	0.007879	0.700876
-40.743266	-1.827157	1.776704	0.007794	0.700881
-40.998843	-1.782174	1.781709	0.007842	0.700880
-41.534329	-1.821299	1.786714	0.007942	0.700606
-41.925981	-1.783352	1.791718	0.008015	0.700542
-42.173237	-1.742777	1.796723	0.008061	0.700534
-41.996161	-1.770982	1.801728	0.008028	0.700541
-41.923378	-1.784630	1.806733	0.008015	0.700539
-42.044001	-1.763943	1.811738	0.008037	0.700538
-41.817712	-1.829067	1.816742	0.007995	0.700487
-42.485298	-1.841706	1.821747	0.008120	0.700220
-42.483897	-1.837430	1.826752	0.008119	0.700229
-43.038356	-1.740259	1.831757	0.008223	0.700225
-43.029671	-1.743516	1.836762	0.008221	0.700221
-42.386067	-1.855998	1.841766	0.008102	0.700226
-43.103576	-1.731443	1.846771	0.008235	0.700219
-43.077246	-1.839694	1.851776	0.008231	0.700009
-43.652759	-1.790274	1.856781	0.008338	0.699900
-43.766061	-1.772929	1.861786	0.008359	0.699894
-43.786679	-1.764805	1.866790	0.008363	0.699903
-44.074187	-1.717431	1.871795	0.008416	0.699895
-43.656648	-1.788755	1.876800	0.008339	0.699901
-43.539628	-1.808523	1.881805	0.008317	0.699903
-44.345645	-1.778514	1.886810	0.008467	0.699672
-44.468471	-1.786883	1.891814	0.008490	0.699611
-44.382200	-1.808665	1.896819	0.008474	0.699597
-44.599506	-1.766081	1.901824	0.008515	0.699605
-44.650566	-1.758104	1.906829	0.008525	0.699602
-44.516659	-1.784230	1.911834	0.008500	0.699598
-44.464893	-1.788824	1.916838	0.008490	0.699607
-45.284370	-1.808896	1.921843	0.008643	0.699269
-45.227481	-1.817519	1.926848	0.008632	0.699272
-45.539318	-1.761612	1.931853	0.008691	0.699272
-45.740684	-1.727597	1.936858	0.008728	0.699268
-45.156969	-1.828947	1.941862	0.008620	0.699274
-45.460766	-1.777778	1.946867	0.008676	0.699267
-45.591758	-1.764038	1.951872	0.008701	0.699248
-46.287305	-1.780231	1.956877	0.008830	0.698963
-46.364266	-1.767442	1.961882	0.008845	0.698960
-46.490107	-1.739674	1.966886	0.008868	0.698971
-46.563902	-1.731520	1.971891	0.008882	0.698961
-46.180574	-1.796636	1.976896	0.008811	0.698967
-46.129077	-1.808677	1.981901	0.008801	0.698961
-46.422706	-1.759934	1.986906	0.008856	0.698954
-46.852231	-1.833337	1.991910	0.008936	0.698648
-47.190337	-1.777772	1.996915	0.008999	0.698639
-46.962549	-1.815368	2.001920	0.008957	0.698645

-47.136230	-1.783498	2.011917	0.008990	0.698646
-47.219426	-1.769843	2.021914	0.009005	0.698643
-47.242842	-1.802136	2.031910	0.009010	0.698569
-47.623341	-1.837950	2.041907	0.009081	0.698357
-48.012968	-1.768948	2.051904	0.009154	0.698356
-47.852638	-1.776631	2.061901	0.009124	0.698398
-47.337801	-1.747493	2.071898	0.009028	0.698644
-47.104872	-1.789374	2.081894	0.008985	0.698643
-47.148923	-1.779701	2.091891	0.008994	0.698646
-46.976811	-1.810850	2.101888	0.008962	0.698644
-47.085675	-1.791348	2.111885	0.008982	0.698644
-47.148059	-1.780789	2.121882	0.008994	0.698643
-47.168150	-1.775736	2.131878	0.008998	0.698645
-46.803868	-1.839237	2.141875	0.008930	0.698648
-47.283325	-1.706814	2.151872	0.009020	0.698743
-46.165375	-1.796677	2.161869	0.008812	0.698965
-46.232878	-1.786629	2.171866	0.008825	0.698961
-46.342525	-1.766565	2.181862	0.008845	0.698961
-46.405032	-1.754292	2.191859	0.008857	0.698963
-45.620584	-1.758859	2.201856	0.008711	0.699238
-45.466931	-1.769940	2.211853	0.008683	0.699270
-45.380614	-1.784979	2.221850	0.008667	0.699271
-45.386793	-1.784445	2.231846	0.008668	0.699269
-44.562038	-1.789745	2.241843	0.008515	0.699557
-44.538936	-1.770143	2.251840	0.008511	0.699604
-44.141854	-1.840450	2.261837	0.008437	0.699605
-44.624602	-1.755233	2.271834	0.008527	0.699603
-43.770030	-1.786073	2.281830	0.008369	0.699849
-43.678629	-1.777216	2.291827	0.008352	0.699900
-43.306317	-1.841679	2.301824	0.008283	0.699903
-43.635663	-1.780162	2.311821	0.008344	0.699908
-42.973451	-1.742848	2.321818	0.008221	0.700223
-42.804268	-1.772972	2.331814	0.008190	0.700223
-42.643232	-1.800448	2.341811	0.008160	0.700225
-42.665936	-1.723596	2.351808	0.008164	0.700372
-41.672301	-1.816290	2.361805	0.007980	0.700543
-42.195828	-1.723230	2.371802	0.008077	0.700542
-41.866111	-1.772266	2.381798	0.008016	0.700562
-41.029472	-1.764743	2.391795	0.007861	0.700879
-40.908088	-1.785918	2.401792	0.007838	0.700879
-40.935478	-1.780716	2.411789	0.007843	0.700880
-40.842645	-1.744649	2.421786	0.007826	0.700986
-40.295840	-1.773129	2.431782	0.007725	0.701125
-40.471425	-1.740537	2.441779	0.007758	0.701127
-40.348288	-1.726717	2.451776	0.007735	0.701200
-39.242973	-1.803970	2.461773	0.007529	0.701442
-39.602925	-1.740818	2.471770	0.007597	0.701439
-39.381713	-1.779445	2.481766	0.007556	0.701441
-38.890336	-1.734858	2.491763	0.007464	0.701708
-38.471201	-1.788811	2.501760	0.007386	0.701749
-38.706099	-1.745990	2.511757	0.007430	0.701751
-38.378102	-1.717717	2.521754	0.007370	0.701926
-37.730323	-1.758844	2.531750	0.007249	0.702076
-37.936042	-1.720493	2.541747	0.007288	0.702079
-37.644366	-1.737485	2.551744	0.007234	0.702149
-36.942324	-1.750767	2.561741	0.007103	0.702375
-36.913576	-1.755808	2.571738	0.007098	0.702375
-36.835536	-1.770565	2.581734	0.007084	0.702373
-36.368708	-1.721527	2.591731	0.006997	0.702640
-35.894897	-1.774947	2.601728	0.006909	0.702702
-35.859563	-1.783289	2.611725	0.006903	0.702698
-35.833722	-1.749135	2.621722	0.006898	0.702776
-34.835506	-1.812213	2.631718	0.006712	0.703007
-35.098278	-1.763263	2.641715	0.006761	0.703011
-34.921126	-1.796196	2.651712	0.006729	0.703008
-34.584397	-1.748411	2.661709	0.006666	0.703225
-34.105092	-1.775296	2.671706	0.006577	0.703343
-34.108740	-1.773864	2.681702	0.006578	0.703344
-34.233577	-1.737275	2.691699	0.006601	0.703373
-33.443964	-1.746785	2.701696	0.006455	0.703638
-33.403217	-1.750828	2.711693	0.006447	0.703644
-33.316189	-1.768661	2.721690	0.006431	0.703639
-32.898649	-1.729524	2.731686	0.006354	0.703867
-32.520911	-1.752462	2.741683	0.006284	0.703956
-32.322946	-1.787904	2.751680	0.006247	0.703956
-32.471902	-1.718018	2.761677	0.006275	0.704043
-31.368422	-1.805988	2.771674	0.006070	0.704262
-31.692509	-1.748860	2.781670	0.006130	0.704260
-31.581442	-1.767995	2.791667	0.006110	0.704261
-30.836830	-1.780043	2.801664	0.005971	0.704504
-30.707080	-1.758608	2.811661	0.005947	0.704593
-30.638153	-1.772324	2.821658	0.005935	0.704590
-30.729971	-1.726470	2.831654	0.005952	0.704649
-29.708679	-1.788896	2.841651	0.005762	0.704889
-29.612276	-1.806114	2.851648	0.005744	0.704889
-29.828444	-1.767220	2.861645	0.005785	0.704889
-29.100444	-1.802542	2.871642	0.005649	0.705079
-29.058925	-1.744415	2.881638	0.005642	0.705211
-28.644850	-1.817023	2.891635	0.005565	0.705213
-28.893256	-1.770907	2.901632	0.005611	0.705216
-28.086261	-1.766517	2.911629	0.005461	0.705514
-28.081024	-1.759948	2.921626	0.005461	0.705529
-28.144239	-1.749682	2.931622	0.005473	0.705526
-27.596830	-1.763981	2.941619	0.005371	0.705693
-27.060268	-1.773062	2.951616	0.005271	0.705867
-27.211168	-1.746271	2.961613	0.005300	0.705866
-26.824740	-1.816472	2.971610	0.005228	0.705863
-26.630278	-1.732478	2.981606	0.005192	0.706102
-26.166273	-1.800492	2.991603	0.005106	0.706131
-26.403250	-1.758552	3.001600	0.005150	0.706130
-25.721201	-1.804706	3.011597	0.005023	0.706281
-25.445258	-1.771761	3.021594	0.004972	0.706446
-25.415711	-1.778149	3.031590	0.004967	0.706443
-25.313608	-1.795371	3.041587	0.004948	0.706445
-24.677546	-1.757310	3.051584	0.004830	0.706748
-24.505551	-1.783293	3.061581	0.004798	0.706757
-24.356631	-1.810727	3.071578	0.004770	0.706755
-24.500757	-1.710940	3.081574	0.004797	0.706904
-23.397674	-1.818426	3.091571	0.004592	0.707082
-23.701974	-1.761881	3.101568	0.004649	0.707086
-23.504782	-1.798308	3.111565	0.004613	0.707083
-22.922294	-1.754172	3.121562	0.004504	0.707380
-22.820005	-1.772008	3.131558	0.004485	0.707380
-22.664925	-1.799294	3.141555	0.004457	0.707381
-22.418472	-1.755384	3.151552	0.004411	0.707557
-21.635736	-1.821885	3.161549	0.004266	0.707703
-21.799349	-1.794158	3.171546	0.004296	0.707699
-21.952192	-1.766013	3.181542	0.004325	0.707701
-21.162251	-1.757504	3.191539	0.004178	0.708000
-21.037733	-1.771038	3.201536	0.004155	0.708017
-20.870174	-1.801638	3.211533	0.004124	0.708015
-20.916996	-1.708570	3.221530	0.004133	0.708184
-19.932045	-1.801055	3.231526	0.003950	0.708350
-20.095236	-1.771222	3.241523	0.003980	0.708351
-20.200786	-1.747762	3.251520	0.004000	0.708360
-19.169091	-1.791164	3.261517	0.003808	0.708641
-19.223095	-1.782001	3.271514	0.003819	0.708640
-18.998648	-1.819423	3.281510	0.003777	0.708645
-19.030732	-1.755050	3.291507	0.003783	0.708762
-18.249644	-1.794533	3.301504	0.003638	0.708961
-18.460953	-1.755695	3.311501	0.003678	0.708963
-18.521630	-1.745422	3.321498	0.003689	0.708962
-17.682173	-1.744433	3.331494	0.003533	0.709263
-17.613313	-1.754004	3.341491	0.003520	0.709268
-17.382040	-1.793147	3.351488	0.003478	0.709271
-17.030275	-1.759122	3.361485	0.003412	0.709465
-16.831196	-1.727632	3.371482	0.003375	0.709598
-16.548968	-1.777963	3.381478	0.003323	0.709598
-16.653846	-1.745005	3.391475	0.003343	0.709626
-15.863907	-1.750321	3.401472	0.003196	0.709896
-15.870724	-1.749218	3.411469	0.003197	0.709896
-15.788413	-1.764506	3.421466	0.003182	0.709894
-15.117749	-1.766341	3.431462	0.003058	0.710129
-14.852975	-1.768980	3.441459	0.003009	0.710217
-14.536466	-1.825340	3.451456	0.002950	0.710217
-14.692464	-1.796087	3.461453	0.002979	0.710220
-14.190835	-1.741644	3.471450	0.002886	0.710507
-13.850305	-1.787690	3.481446	0.002823	0.710535
-14.027580	-1.755780	3.491443	0.002856	0.710536
-13.719759	-1.739804	3.501440	0.002799	0.710677
-12.891486	-1.787708	3.511437	0.002645	0.710875
-12.832312	-1.798404	3.521434	0.002634	0.710875
-13.019438	-1.767088	3.531430	0.002669	0.710870
-12.533796	-1.754179	3.541427	0.002579	0.711068
-12.096756	-1.794578	3.551424	0.002498	0.711143
-12.258612	-1.764791	3.561421	0.002528	0.711144
-12.160996	-1.730209	3.571418	0.002510	0.711248
-11.083101	-1.816119	3.581414	0.002310	0.711459
-11.378700	-1.762538	3.591411	0.002365	0.711460
-11.261261	-1.783186	3.601408	0.002343	0.711460
-10.736586	-1.750491	3.611405	0.002246	0.711712
-10.359102	-1.789607	3.621402	0.002176	0.711767
-10.584347	-1.750093	3.631398	0.002218	0.711766
-10.371158	-1.728138	3.641395	0.002178	0.711885
-9.668053	-1.747784	3.651392	0.002047	0.712095
-9.653704	-1.748611	3.661389	0.002045	0.712098
-9.736096	-1.721022	3.671386	0.002061	0.712123
-8.678705	-1.775864	3.681382	0.001864	0.712389
-8.595298	-1.789818	3.691379	0.001849	0.712391
-8.035353	-1.888801	3.701376	0.001745	0.712392
-8.503985	-1.770727	3.711373	0.001832	0.712460
-7.196820	-1.875811	3.721370	0.001589	0.712714
-7.623255	-1.801317	3.731366	0.001668	0.712711
-7.336235	-1.853277	3.741363	0.001615	0.712709
-7.259091	-1.836124	3.751360	0.001601	0.712770
-6.540090	-1.835484	3.761357	0.001467	0.713026
-6.361379	-1.867125	3.771354	0.001434	0.713026
-6.619445	-1.821178	3.781350	0.001483	0.713025
-6.641933	-1.764226	3.791347	0.001487	0.713130
-5.403966	-1.867296	3.801344	0.001257	0.713364
-5.685347	-1.816686	3.811341	0.001309	0.713364
-5.561060	-1.838315	3.821338	0.001286	0.713365
-5.066242	-1.835620	3.831334	0.001194	0.713545
-4.691582	-1.848954	3.841331	0.001125	0.713651
-4.587657	-1.866915	3.851328	0.001106	0.713652
-4.598730	-1.863091	3.861325	0.001108	0.713655
-3.781013	-1.880845	3.871322	0.000956	0.713909
-3.936775	-1.821356	3.881318	0.000985	0.713972
-3.703347	-1.863411	3.891315	0.000942	0.713970
-3.724541	-1.848226	3.901312	0.000946	0.713993
-3.305962	-1.776943	3.911309	0.000868	0.714282
-2.919980	-1.847357	3.921306	0.000797	0.714278
-3.021061	-1.829147	3.931302	0.000816	0.714278
-2.741911	-1.764290	3.941299	0.000764	0.714505
-2.039660	-1.835238	3.951296	0.000633	0.714613
-1.885712	-1.863526	3.961293	0.000605	0.714610
-2.147262	-1.788466	3.971290	0.000654	0.714667
-1.376588	-1.803035	3.981286	0.000511	0.714910
-1.696320	-1.746977	3.991283	0.000570	0.714908
-1.305531	-1.814465	4.001280	0.000498	0.714911
-1.007678	-1.709419	4.011277	0.000442	0.715225
-0.929395	-1.718278	4.021274	0.000428	0.715234
-0.907700	-1.719066	4.031270	0.000424	0.715240
-0.729046	-1.594799	4.041267	0.000391	0.715549
-0.778230	-1.586585	4.051264	0.000400	0.715548
-0.776319	-1.491209	4.061261	0.000400	0.715737
-0.615289	-1.445409	4.071258	0.000370	0.715884
-0.467390	-1.420996	4.081254	0.000343	0.715985
-0.586135	-1.324739	4.091251	0.000365	0.716133
-0.465143	-1.272356	4.101248	0.000343	0.716279
-0.452416	-1.188399	4.111245	0.000341	0.716449
-0.373891	-1.097351	4.121242	0.000326	0.716657
-0.338506	-1.048774	4.131238	0.000320	0.716765
-0.180203	-0.915804	4.141235	0.000291	0.717084
-0.374935	-0.805542	4.151232	0.000327	0.717233
-0.185572	-0.751589	4.161229	0.000292	0.717406
-0.223532	-0.591462	4.171226	0.000299	0.717709
-0.202234	-0.484974	4.181222	0.000295	0.717926
0.006219	-0.407949	4.191219	0.000257	0.718151
0.140026	-0.309915	4.201216	0.000232	0.718392
0.151037	-0.181537	4.211213	0.000230	0.718649
0.136533	-0.036688	4.221210	0.000233	0.718929
0.102435	0.102119	4.231206	0.000239	0.719191
0.110106	0.244116	4.241203	0.000238	0.719473
0.000000	0.432758	4.251200	0.000258	0.719806

0.292378	1.004664	4.256205	0.000204	0.721034
0.503591	2.217980	4.261210	0.000164	0.723491
0.855062	4.008116	4.266214	0.000097	0.727115
1.090904	6.368983	4.271219	0.000052	0.731788
1.738222	9.174582	4.276224	-0.000070	0.737428
2.001051	12.515942	4.281229	-0.000121	0.743918
2.358732	16.302712	4.286234	-0.000190	0.751224
2.633197	20.511215	4.291238	-0.000244	0.759221
2.978651	25.090800	4.296243	-0.000311	0.767843
3.659594	29.999970	4.301248	-0.000441	0.777081
4.028039	35.296971	4.306253	-0.000513	0.786809
4.231985	40.954746	4.311258	-0.000555	0.797008
4.700856	46.850936	4.316262	-0.000646	0.807580
5.433369	52.993633	4.321267	-0.000786	0.818523
6.240015	59.403580	4.326272	-0.000940	0.829801
6.889784	66.063749	4.331277	-0.001065	0.841302
8.526921	72.785981	4.336282	-0.001375	0.853041
9.928983	79.776975	4.341286	-0.001640	0.864992
10.540017	87.094170	4.346291	-0.001759	0.877082
11.135860	94.593315	4.351296	-0.001874	0.889293
11.818825	102.227820	4.356301	-0.002006	0.901575
12.822527	109.966566	4.361306	-0.002198	0.913941
13.777820	117.828280	4.366310	-0.002381	0.926317
14.310182	125.883234	4.371315	-0.002485	0.938709
15.091941	134.010577	4.376320	-0.002636	0.951112
15.831323	142.208411	4.381325	-0.002779	0.963448
16.552997	150.515337	4.386330	-0.002919	0.975782
17.408785	158.871124	4.391334	-0.003083	0.988064
18.184842	167.291599	4.396339	-0.003233	1.000268
19.028262	175.742752	4.401344	-0.003396	1.012383
19.676979	184.264981	4.406349	-0.003522	1.024406
20.232577	192.849049	4.411354	-0.003631	1.036352
20.866657	201.437438	4.416358	-0.003754	1.048186
21.583142	210.042289	4.421363	-0.003893	1.059928
22.675319	218.626176	4.426368	-0.004102	1.071599
22.978819	227.317105	4.431373	-0.004164	1.083106
23.584459	235.983758	4.436378	-0.004283	1.094528
24.563285	244.581727	4.441382	-0.004470	1.105825
25.215209	253.237542	4.446387	-0.004597	1.117010
25.832165	261.884793	4.451392	-0.004718	1.128066
26.557423	270.517745	4.456397	-0.004858	1.139019
27.450318	279.143176	4.461402	-0.005030	1.149893
28.069627	287.804952	4.466406	-0.005151	1.160653
28.949938	296.386765	4.471411	-0.005320	1.171270
29.541387	305.018192	4.476416	-0.005436	1.181792
30.039589	313.656169	4.481421	-0.005534	1.192210
30.962506	322.200509	4.486426	-0.005711	1.202512
31.617263	330.789715	4.491430	-0.005839	1.212725
32.282875	339.352241	4.496435	-0.005968	1.222824
32.916526	347.947959	4.501440	-0.006092	1.232871
33.358997	356.507747	4.506445	-0.006180	1.242759
34.021283	365.050969	4.511450	-0.006308	1.252593
34.301408	373.620287	4.516454	-0.006366	1.262306
35.015689	382.110957	4.521459	-0.006505	1.271938
35.671557	390.596164	4.526464	-0.006632	1.281482
35.819708	399.140310	4.531469	-0.006665	1.290925
36.324615	407.633757	4.536474	-0.006765	1.300309
37.175963	416.088836	4.541478	-0.006928	1.309648
37.583837	424.643362	4.546483	-0.007010	1.318947
37.972326	433.072165	4.551488	-0.007088	1.328043
38.542215	441.458993	4.556493	-0.007199	1.337064
39.240027	449.818590	4.561498	-0.007334	1.346019
39.668442	458.242790	4.566502	-0.007420	1.354935
40.065494	466.634160	4.571507	-0.007499	1.363753
40.742087	475.000011	4.576512	-0.007630	1.372535
41.267162	483.355400	4.581517	-0.007733	1.381225
41.927875	491.711766	4.586522	-0.007862	1.389885
42.594602	500.059479	4.591526	-0.007991	1.398482
43.006909	508.403992	4.596531	-0.008073	1.406982
43.433930	516.778200	4.601536	-0.008158	1.415462
43.947900	525.090783	4.606541	-0.008259	1.423844
44.559919	533.415845	4.611546	-0.008378	1.432206
44.900064	541.751382	4.616550	-0.008447	1.440485
45.432741	550.048356	4.621555	-0.008552	1.448709
46.005475	558.370980	4.626560	-0.008663	1.456919
46.451555	566.658112	4.631565	-0.008752	1.465028
46.775544	575.043839	4.636570	-0.008818	1.473167
47.378691	583.298874	4.641574	-0.008935	1.481181
48.051123	591.537944	4.646579	-0.009066	1.489146
48.405674	599.860179	4.651584	-0.009137	1.497099
48.733047	608.132488	4.656589	-0.009203	1.504958
49.413798	616.392583	4.661594	-0.009335	1.512819
49.936624	624.632829	4.666598	-0.009438	1.520596
50.289564	632.896304	4.671603	-0.009509	1.528329
50.927972	641.147140	4.676608	-0.009633	1.536055
51.264821	649.401872	4.681613	-0.009701	1.543700
51.522241	657.687973	4.686618	-0.009754	1.551325
51.978383	665.931701	4.691622	-0.009844	1.558902
52.357815	674.152440	4.696627	-0.009920	1.566411
53.110480	682.353058	4.701632	-0.010066	1.573920
53.508904	690.571452	4.706637	-0.010145	1.581358
54.199927	698.771967	4.711642	-0.010279	1.588787
54.252148	707.072261	4.716646	-0.010294	1.596179
54.545762	715.293572	4.721651	-0.010354	1.603501
54.849277	723.537065	4.726656	-0.010416	1.610810
55.115776	731.763002	4.731661	-0.010471	1.618066
55.501579	739.955009	4.736666	-0.010548	1.625276
56.077018	748.186845	4.741670	-0.010660	1.632515
56.419665	756.383045	4.746675	-0.010729	1.639659
56.996844	764.542277	4.751680	-0.010842	1.646772
57.233504	772.756522	4.756685	-0.010891	1.653856
57.674853	780.922853	4.761690	-0.010979	1.660895
58.124582	789.107953	4.766694	-0.011067	1.667922
58.379060	797.326040	4.771699	-0.011120	1.674922
59.030778	805.462685	4.776704	-0.011247	1.681876
59.366859	813.642748	4.781709	-0.011314	1.688796
59.645529	821.859855	4.786714	-0.011372	1.695711
60.133393	830.022281	4.791718	-0.011468	1.702579
60.603174	838.191305	4.796723	-0.011560	1.709423
61.097239	846.390907	4.801728	-0.011658	1.716268
61.336731	854.556920	4.806733	-0.011707	1.723026
61.691489	862.727448	4.811738	-0.011779	1.729775
62.259837	870.878028	4.816742	-0.011890	1.736509
62.709724	879.023510	4.821747	-0.011979	1.743197
63.267872	887.173028	4.826752	-0.012088	1.749877
63.490515	895.370699	4.831757	-0.012134	1.756527
63.909518	903.520668	4.836762	-0.012218	1.763139
64.198745	911.695769	4.841766	-0.012277	1.769730
64.615369	919.847379	4.846771	-0.012360	1.776293
64.962806	928.012828	4.851776	-0.012429	1.782835
65.262385	936.183134	4.856781	-0.012490	1.789350
65.800249	944.356688	4.861786	-0.012596	1.795874
66.181080	952.469613	4.866790	-0.012672	1.802307
66.531103	960.613097	4.871795	-0.012742	1.808737
66.973021	968.762725	4.876800	-0.012830	1.815160
67.249307	976.904983	4.881805	-0.012886	1.821534
67.679398	985.028984	4.886810	-0.012972	1.827891
68.333703	993.157910	4.891814	-0.013099	1.834256
68.603796	1001.292390	4.896819	-0.013154	1.840557
69.034195	1009.438973	4.901824	-0.013240	1.846865
69.114258	1017.622395	4.906829	-0.013260	1.853139
69.621231	1025.730376	4.911834	-0.013359	1.859383
70.156271	1033.838163	4.916838	-0.013464	1.865610
70.620178	1041.982351	4.921843	-0.013556	1.871835
70.956676	1050.134195	4.926848	-0.013624	1.878031
71.226835	1058.251942	4.931853	-0.013679	1.884172
71.614864	1066.383726	4.936858	-0.013756	1.890318
71.797463	1074.555155	4.941862	-0.013796	1.896450
72.239491	1082.638988	4.946867	-0.013883	1.902526
72.590049	1090.791342	4.951872	-0.013954	1.908623
72.694774	1098.945877	4.956877	-0.013978	1.914675
72.975280	1107.063980	4.961882	-0.014036	1.920701
73.513712	1115.158510	4.966886	-0.014141	1.926719
73.652122	1123.309304	4.971891	-0.014172	1.932715
74.094719	1131.426940	4.976896	-0.014260	1.938701
74.564912	1139.498605	4.981901	-0.014352	1.944639
75.073414	1147.635850	4.986906	-0.014452	1.950610
75.506053	1155.772978	4.991910	-0.014538	1.956554
75.554516	1163.884807	4.996915	-0.014552	1.962421
76.015013	1171.970423	5.001920	-0.014643	1.968295
76.257270	1180.099704	5.006925	-0.014694	1.974160
76.738312	1188.163195	5.011930	-0.014788	1.979986
77.356452	1196.235472	5.016934	-0.014909	1.985815
77.607861	1204.371628	5.021939	-0.014961	1.991634
77.867864	1212.507408	5.026944	-0.015014	1.997437
78.351936	1220.573319	5.031949	-0.015109	2.003196
78.608975	1228.697167	5.036954	-0.015162	2.008956
78.812119	1236.848316	5.041958	-0.015205	2.014713
79.168285	1244.921938	5.046963	-0.015277	2.020416
79.437474	1253.049162	5.051968	-0.015332	2.026130
79.692281	1261.175925	5.056973	-0.015385	2.031827
80.071198	1269.283866	5.061978	-0.015461	2.037507
80.566229	1277.336411	5.066982	-0.015558	2.043145
80.819684	1285.430356	5.071987	-0.015610	2.048771
81.073648	1293.579318	5.076992	-0.015663	2.054419
81.342495	1301.652891	5.081997	-0.015718	2.060002
81.856909	1309.712012	5.087002	-0.015819	2.065584
82.199990	1317.831848	5.092006	-0.015888	2.071176
82.751728	1325.895632	5.097011	-0.015996	2.076735
83.195441	1333.971254	5.102016	-0.016084	2.082276
83.456205	1342.074866	5.107021	-0.016137	2.087803
83.724364	1350.211796	5.112026	-0.016193	2.093339
83.976620	1358.322805	5.117030	-0.016245	2.098842
84.391212	1366.383998	5.122035	-0.016327	2.104312
84.737505	1374.508721	5.127040	-0.016397	2.109803
85.197256	1382.635479	5.132045	-0.016488	2.115293
85.507617	1390.694876	5.137050	-0.016550	2.120709
85.934912	1398.764618	5.142054	-0.016635	2.126129
86.073757	1406.886442	5.147059	-0.016666	2.131543
86.510760	1414.979608	5.152064	-0.016753	2.136952
86.753806	1423.049860	5.157069	-0.016803	2.142314
86.944737	1431.150126	5.162074	-0.016844	2.147677
87.519668	1439.221091	5.167078	-0.016956	2.153043
87.860664	1447.276075	5.172083	-0.017025	2.158364
88.176461	1455.367447	5.177088	-0.017089	2.163693
88.498694	1463.453940	5.182093	-0.017154	2.169006
88.902060	1471.535543	5.187098	-0.017234	2.174311
89.318344	1479.610841	5.192102	-0.017317	2.179599
89.475584	1487.701860	5.197107	-0.017351	2.184861
90.125494	1495.772909	5.202112	-0.017477	2.190143
90.183962	1503.920976	5.207117	-0.017494	2.195407
90.520120	1511.975394	5.212122	-0.017561	2.200624
90.863334	1520.044052	5.217126	-0.017630	2.205838
91.061410	1528.129590	5.222131	-0.017672	2.211037
91.535198	1536.216548	5.227136	-0.017766	2.216250
91.763757	1544.284832	5.232141	-0.017813	2.221416
92.210363	1552.346151	5.237146	-0.017902	2.226586
92.328748	1560.478927	5.242150	-0.017929	2.231760
92.583504	1568.547442	5.247155	-0.017982	2.236893
93.195419	1576.587010	5.252160	-0.018101	2.242027
93.363917	1584.676092	5.257165	-0.018137	2.247142
93.705744	1592.765053	5.262170	-0.018206	2.252260
94.271325	1600.816391	5.267174	-0.018316	2.257363
94.673000	1608.859217	5.272179	-0.018396	2.262434
95.014003	1616.957067	5.277184	-0.018465	2.267523
95.128675	1625.127029	5.282189	-0.018492	2.272625
95.521113	1633.185565	5.287194	-0.018570	2.277671
95.759652	1641.246502	5.292198	-0.018619	2.282694
96.067416	1649.290082	5.297203	-0.018682	2.287701
96.445862	1657.373388	5.302208	-0.018757	2.292728
96.996008	1665.401663	5.307213	-0.018865	2.297724
97.425491	1673.459807	5.312218	-0.018950	2.302717
97.738875	1681.536909	5.317222	-0.019014	2.307702
97.834374	1689.658995	5.322227	-0.019037	2.312684
98.092159	1697.743496	5.327232	-0.019090	2.317647
98.411261	1705.781537	5.332237	-0.019154	2.322576
98.904648	1713.819017	5.337242	-0.019251	2.327508
99.120281	1721.927676	5.342246	-0.019297	2.332450
99.345780	1729.983240	5.347251	-0.019344	2.337350
99.847505	1738.048598	5.352256	-0.019442	2.342269
100.162129	1746.106653	5.357261	-0.019506	2.347157
100.433104	1754.213849	5.362266	-0.019562	2.352061
100.648740	1762.295455	5.367270	-0.019607	2.356935
101.060100	1770.303160	5.372275	-0.019689	2.361770
101.515414	1778.353752	5.377280	-0.019779	2.366625
101.465413	1786.476132	5.382285	-0.019775	2.371471
101.808908	1794.535994	5.387290	-0.019844	2.376303
102.173068	1802.597114	5.392294	-0.019917	2.381126
102.311692	1810.656624	5.397299	-0.019948	2.385921
102.672098	1818.742334	5.402304	-0.020020	2.390740
102.892155	1826.818429	5.407309	-0.020066	2.395531
103.288580	1834.841498	5.412314	-0.020145	2.400296
103.614773	1842.900488	5.417318	-0.020211	2.405067
104.162740	1850.928116	5.422323	-0.020318	2.409827
104.413316	1859.053327	5.427328	-0.020370	2.414612
104.489093	1867.112038	5.432333	-0.020389	2.419335
104.941026	1875.144752	5.437338	-0.020478	2.424062
105.223864	1883.232701	5.442342	-0.020536	2.428800
105.674800	1891.344242	5.447347	-0.020625	2.433554
106.236615	1899.378767	5.452352	-0.020735	2.438263
106.344078	1907.437808	5.457357	-0.020760	2.442943
106.537973	1915.495884	5.462362	-0.020801	2.447619
106.637422	1923.587859	5.467366	-0.020825	2.452299
107.121393	1931.581786	5.472371	-0.020920	2.456943
107.548867	1939.622455	5.477376	-0.021005	2.461600
107.737196	1947.697100	5.482381	-0.021045	2.466250
107.945538	1955.781776	5.487386	-0.021089	2.470898
108.701321	1963.802560	5.492390	-0.021235	2.475542
108.788806	1971.854416	5.497395	-0.021257	2.480145
109.002752	1979.939965	5.502400	-0.021302	2.484768
109.381407	1987.976496	5.507405	-0.021377	2.489367
109.751680	1996.053716	5.512410	-0.021451	2.493979
110.145361	2004.106986	5.517414	-0.021530	2.498572
110.295344	2012.162324	5.522419	-0.021563	2.503139
110.792686	2020.218961	5.527424	-0.021661	2.507723
110.853356	2028.329138	5.532429	-0.021677	2.512298
111.445031	2036.358109	5.537434	-0.021792	2.516857
111.920055	2044.378311	5.542438	-0.021886	2.521394
111.809217	2052.469948	5.547443	-0.021870	2.525921
112.324761	2060.519069	5.552448	-0.021972	2.530461
112.640994	2068.586898	5.557453	-0.022036	2.534989
112.961119	2076.615048	5.562458	-0.022100	2.539487
112.963687	2084.695560	5.567462	-0.022106	2.543984
113.463093	2092.708909	5.572467	-0.022204	2.548471
113.902500	2100.791089	5.577472	-0.022291	2.552983
114.074776	2108.839294	5.582477	-0.022328	2.557450
114.234394	2116.890846	5.587482	-0.022363	2.561910
114.659355	2124.940275	5.592486	-0.022447	2.566379
114.915669	2133.009115	5.597491	-0.022500	2.570840
115.238750	2141.077752	5.602496	-0.022566	2.575297
115.369813	2149.115825	5.607501	-0.022595	2.579717
115.914786	2157.132321	5.612506	-0.022702	2.584145
116.143777	2165.230538	5.617510	-0.022750	2.588589
116.079856	2173.454774	5.622515	-0.022743	2.593074
116.434358	2181.505578	5.627520	-0.022814	2.597485
116.671151	2189.481884	5.632525	-0.022863	2.601840
116.817420	2197.516644	5.637530	-0.022896	2.606214
117.278514	2205.529277	5.642534	-0.022987	2.610589
117.446708	2213.583659	5.647539	-0.023023	2.614960
117.783162	2221.596346	5.652544	-0.023091	2.619312
118.031920	2229.630825	5.657549	-0.023142	2.623663
118.339290	2237.663717	5.662554	-0.023205	2.628010
118.518372	2245.739596	5.667558	-0.023243	2.632363
118.694204	2253.790069	5.672563	-0.023281	2.636696
119.046713	2261.841481	5.677568	-0.023352	2.641034
119.365220	2269.850957	5.682573	-0.023416	2.645340
119.572772	2277.903085	5.687578	-0.023460	2.649655
120.093175	2285.965305	5.692582	-0.023562	2.653988
120.283071	2294.001912	5.697587	-0.023603	2.658279
120.395255	2302.074632	5.702592	-0.023629	2.662577
120.782639	2310.109848	5.707597	-0.023706	2.666866
121.048034	2318.189006	5.712602	-0.023760	2.671163
121.299946	2326.265256	5.717606	-0.023813	2.675451
121.475975	2334.278036	5.722611	-0.023850	2.679694
121.857360	2342.309567	5.727616	-0.023927	2.683953
122.031195	2350.361378	5.732621	-0.023964	2.688203
122.483738	2358.403092	5.737626	-0.024053	2.692458
122.669391	2366.480442	5.742630	-0.024093	2.696708
123.037233	2374.504000	5.747635	-0.024167	2.700935
123.064126	2382.573547	5.752640	-0.024177	2.705158
123.254425	2390.611000	5.757645	-0.024218	2.709368
123.692475	2398.657765	5.762650	-0.024304	2.713591
123.933467	2406.718084	5.767654	-0.024354	2.717803
123.899054	2414.750601	5.772659	-0.024353	2.721976
124.386674	2422.774156	5.777664	-0.024449	2.726171
124.521839	2430.837820	5.782669	-0.024479	2.730358
124.545005	2438.912760	5.787674	-0.024489	2.734538
124.904528	2446.932977	5.792678	-0.024561	2.738704
125.125334	2454.966899	5.797683	-0.024607	2.742862
125.452193	2463.007889	5.802688	-0.024673	2.747023
125.639198	2471.084452	5.807693	-0.024713	2.751188
126.036624	2479.177177	5.812698	-0.024792	2.755368
126.401608	2487.160105	5.817702	-0.024865	2.759483
126.510135	2495.177340	5.822707	-0.024891	2.763594
126.856281	2503.216622	5.827712	-0.024960	2.767725
126.968682	2511.272211	5.832717	-0.024986	2.771843
127.163658	2519.343078	5.837722	-0.025028	2.775968
127.571309	2527.355220	5.842726	-0.025109	2.780070
127.834484	2535.364897	5.847731	-0.025163	2.784156
128.240079	2543.414273	5.852736	-0.025243	2.788264
128.176921	2551.489455	5.857741	-0.025237	2.792352
128.345984	2559.553862	5.862746	-0.025273	2.796441
128.668429	2567.579659	5.867750	-0.025339	2.800515
128.554271	2575.618812	5.872755	-0.025323	2.804563
129.102815	2583.650199	5.877760	-0.025430	2.808641
129.509100	2591.678263	5.882765	-0.025511	2.812702
129.504456	2599.768480	5.887770	-0.025515	2.816765
129.635934	2607.807428	5.892774	-0.025544	2.820804
130.106936	2615.796026	5.897779	-0.025637	2.824832
130.480219	2623.851818	5.902784	-0.025712	2.828882
130.533071	2631.952176	5.907789	-0.025727	2.832930
130.859313	2639.967230	5.912794	-0.025793	2.836945
131.182818	2648.001041	5.917798	-0.025858	2.840964
131.204373	2656.019739	5.922803	-0.025867	2.844952
131.500012	2664.073392	5.927808	-0.025927	2.848968
131.602232	2672.137143	5.932813	-0.025952	2.852972
131.833085	2680.159902	5.937818	-0.026000	2.856957
132.303956	2688.185895	5.942822	-0.026093	2.860951
132.601269	2696.191650	5.947827	-0.026153	2.864921
132.934574	2704.250888	5.952832	-0.026220	2.868913
133.036742	2712.310661	5.957837	-0.026244	2.872887
133.355521	2720.343429	5.962842	-0.026309	2.876854
133.550212	2728.394970	5.967846	-0.026350	2.880818
133.679143	2736.405796	5.972851	-0.026379	2.884753
134.068503	2744.471368	5.977856	-0.026457	2.888723
134.628598	2752.484554	5.982861	-0.026566	2.892672
134.563098	2760.555391	5.987866	-0.026559	2.896610
134.678808	2768.627359	5.992870	-0.026586	2.900552
135.101816	2776.589149	5.997875	-0.026670	2.904452
135.598987	2784.660969	6.002880	-0.026768	2.908404
135.791275	2792.777641	6.007885	-0.026809	2.912356
136.092069	2800.832965	6.012890	-0.026870	2.916279
136.254387	2808.837106	6.017894	-0.026905	2.920165
137.323861	2816.744175	6.022899	-0.027109	2.924046
137.842756	2824.773015	6.027904	-0.027211	2.927951
138.003881	2832.844812	6.032909	-0.027246	2.931854
138.208858	2840.910354	6.037914	-0.027290	2.935750
138.348207	2848.953609	6.042918	-0.027321	2.939627
138.613181	2856.969860	6.047923	-0.027375	2.943492
138.992945	2865.018857	6.052928	-0.027451	2.947374
138.924784	2873.108903	6.057933	-0.027443	2.951247
139.158899	2881.154041	6.062938	-0.027492	2.955109
139.441536	2889.168652	6.067942	-0.027550	2.958954
139.732089	2897.166813	6.072947	-0.027609	2.962787
140.032138	2905.221656	6.077952	-0.027670	2.966642
140.474424	2913.248262	6.082957	-0.027758	2.970486
140.590500	2921.305320	6.087962	-0.027784	2.974323
140.752701	2929.369236	6.092966	-0.027820	2.978160
140.794918	2937.412967	6.097971	-0.027833	2.981976
141.223608	2945.424560	6.102976	-0.027918	2.985792
141.463296	2953.456817	6.107981	-0.027967	2.989604
141.554044	2961.538404	6.112986	-0.027990	2.993426
141.930801	2969.559698	6.117990	-0.028065	2.997229
141.983117	2977.592528	6.122995	-0.028080	3.001017
142.109510	2985.602500	6.128000	-0.028108	3.004793
142.519660	2993.615335	6.133005	-0.028190	3.008579
142.679212	3001.676142	6.138010	-0.028225	3.012371
142.983399	3009.750011	6.143014	-0.028286	3.016171
143.010860	3017.754458	6.148019	-0.028297	3.019920
143.453833	3025.760843	6.153024	-0.028384	3.023686
143.775295	3033.798151	6.158029	-0.028449	3.027455
143.930861	3041.837479	6.163034	-0.028483	3.031213
144.416341	3049.888786	6.168038	-0.028579	3.034987
144.504303	3057.913068	6.173043	-0.028600	3.038725
144.793249	3065.962769	6.178048	-0.028659	3.042480
145.036996	3073.976765	6.183053	-0.028710	3.046212
145.277105	3082.015920	6.188058	-0.028760	3.049950
145.511428	3090.087930	6.193062	-0.028808	3.053699
145.645602	3098.078951	6.198067	-0.028839	3.057400
145.945050	3106.137176	6.203072	-0.028899	3.061136
146.299504	3114.130704	6.208077	-0.028971	3.064841
146.434041	3122.197923	6.213082	-0.029001	3.068564
146.673834	3130.297543	6.218086	-0.029051	3.072303
146.970263	3138.357217	6.223091	-0.029111	3.076021
147.240562	3146.337593	6.228096	-0.029166	3.079697
147.368504	3154.365249	6.233101	-0.029195	3.083384
147.494320	3162.375515	6.238106	-0.029224	3.087058
147.651888	3170.437945	6.243110	-0.029258	3.090753
147.793908	3178.455611	6.248115	-0.029290	3.094423
148.273919	3186.482405	6.253120	-0.029384	3.098108
148.354447	3194.512523	6.258125	-0.029405	3.101771
148.488860	3202.536489	6.263130	-0.029435	3.105430
148.850404	3210.574063	6.268134	-0.029507	3.109102
148.942010	3218.635213	6.273139	-0.029529	3.112767
148.985897	3226.684505	6.278144	-0.029543	3.116420
149.284081	3234.643519	6.283149	-0.029603	3.120040
149.687868	3242.673925	6.288154	-0.029684	3.123692
149.761842	3250.739016	6.293158	-0.029702	3.127341
149.962005	3258.746435	6.298163	-0.029745	3.130966
150.195442	3266.824376	6.303168	-0.029793	3.134619
150.414621	3274.821730	6.308173	-0.029839	3.138231
150.805925	3282.833714	6.313178	-0.029917	3.141853
151.065031	3290.875761	6.318182	-0.029971	3.145479
151.342101	3298.897630	6.323187	-0.030027	3.149092
151.603810	3306.981915	6.328192	-0.030081	3.152728
151.769412	3315.020872	6.333197	-0.030117	3.156336
152.080480	3323.026330	6.338202	-0.030180	3.159930
152.174174	3331.044700	6.343206	-0.030203	3.163517
152.342894	3339.057253	6.348211	-0.030239	3.167101
152.763862	3347.093109	6.353216	-0.030323	3.170701
152.769381	3355.184035	6.358221	-0.030329	3.174304
152.911091	3363.188875	6.363226	-0.030361	3.177871
153.431967	3371.213435	6.368230	-0.030463	3.181458
153.546153	3379.222993	6.373235	-0.030489	3.185018
153.590537	3387.291244	6.378240	-0.030503	3.188596
153.805641	3395.333930	6.383245	-0.030548	3.192167
154.105106	3403.372039	6.388250	-0.030609	3.195734
154.317882	3411.380164	6.393254	-0.030653	3.199281
154.374428	3419.409295	6.398259	-0.030669	3.202827
154.831935	3427.424943	6.403264	-0.030759	3.206379
155.116859	3435.448304	6.408269	-0.030818	3.209924
155.292668	3443.501634	6.413274	-0.030855	3.213474
155.452265	3451.553402	6.418278	-0.030890	3.217018
155.450506	3459.571649	6.423283	-0.030895	3.220537
155.813311	3467.559483	6.428288	-0.030968	3.224053
156.093440	3475.598203	6.433293	-0.031025	3.227585
156.339143	3483.644805	6.438298	-0.031076	3.231114
156.345116	3491.770581	6.443302	-0.031082	3.234665
156.466156	3499.749305	6.448307	-0.031110	3.238152
156.751659	3507.749369	6.453312	-0.031168	3.241652
156.826891	3515.746862	6.458317	-0.031187	3.245138
157.137916	3523.772127	6.463322	-0.031250	3.248642
157.400004	3531.822950	6.468326	-0.031304	3.252151
157.483442	3539.870986	6.473331	-0.031325	3.255648
157.562506	3547.892827	6.478336	-0.031345	3.259129
157.743986	3555.916066	6.483341	-0.031384	3.262612
158.242540	3563.911028	6.488346	-0.031482	3.266091
158.524728	3571.952581	6.493350	-0.031539	3.269578
158.451562	3580.027995	6.498355	-0.031531	3.273062
158.843215	3588.074808	6.503360	-0.031609	3.276548
159.102779	3596.042317	6.508365	-0.031662	3.279991
159.602927	3604.056797	6.513370	-0.031761	3.283460
159.709913	3612.121317	6.518374	-0.031786	3.286931
159.709788	3620.155344	6.523379	-0.031791	3.290382
159.824214	3628.231195	6.528384	-0.031817	3.293851
160.131564	3636.231989	6.533389	-0.031880	3.297292
160.237445	3644.222851	6.538394	-0.031904	3.300717
160.607280	3652.249617	6.543398	-0.031978	3.304164
160.670206	3660.278676	6.548403	-0.031995	3.307596
160.910578	3668.336192	6.553408	-0.032045	3.311044
161.234783	3676.383069	6.558413	-0.032111	3.314487
161.343024	3684.395991	6.563418	-0.032136	3.317904
161.542094	3692.431232	6.568422	-0.032178	3.321330
161.778232	3700.384880	6.573427	-0.032227	3.324719
162.047280	3708.430682	6.578432	-0.032282	3.328145
162.054741	3716.498296	6.583437	-0.032289	3.331567
162.386877	3724.509657	6.588442	-0.032356	3.334974
162.824544	3732.523845	6.593446	-0.032442	3.338382
163.052571	3740.534428	6.598451	-0.032490	3.341778
163.307020	3748.556153	6.603456	-0.032543	3.345176
163.567370	3756.605636	6.608461	-0.032596	3.348582
163.692315	3764.677396	6.613466	-0.032625	3.351989
163.807339	3772.747165	6.618470	-0.032651	3.355391
163.830170	3780.726956	6.623475	-0.032660	3.358749
164.147547	3788.760022	6.628480	-0.032725	3.362136
164.209092	3796.779407	6.633485	-0.032741	3.365505
164.234174	3804.804772	6.638490	-0.032751	3.368872
164.581958	3812.877711	6.643494	-0.032821	3.372267
164.701300	3820.903802	6.648499	-0.032848	3.375630
165.031748	3828.884900	6.653504	-0.032915	3.378979
165.280308	3836.938604	6.658509	-0.032966	3.382352
165.186833	3844.966552	6.663514	-0.032954	3.385699
165.605634	3852.974124	6.668518	-0.033037	3.389052
165.723215	3861.054214	6.673523	-0.033064	3.392421
165.929619	3869.142440	6.678528	-0.033108	3.395794
165.889804	3877.071590	6.683533	-0.033105	3.399088
166.026539	3885.090682	6.688538	-0.033136	3.402423
166.400243	3893.112233	6.693542	-0.033211	3.405763
166.498053	3901.100006	6.698547	-0.033234	3.409077
166.589700	3909.190419	6.703552	-0.033256	3.412430
166.942709	3917.218840	6.708557	-0.033327	3.415763
167.228591	3925.170872	6.713562	-0.033385	3.419058
167.333065	3933.245564	6.718566	-0.033410	3.422395
167.479719	3941.237619	6.723571	-0.033443	3.425696
167.723661	3949.259793	6.728576	-0.033493	3.429009
167.868934	3957.328287	6.733581	-0.033525	3.432335
168.001420	3965.360150	6.738586	-0.033555	3.435642
168.373867	3973.366568	6.743590	-0.033630	3.438944
168.442282	3981.384283	6.748595	-0.033647	3.442236
168.645096	3989.423946	6.753600	-0.033690	3.445540
168.868187	3997.471310	6.758605	-0.033737	3.448843
168.922812	4005.492020	6.763610	-0.033752	3.452127
169.285153	4013.541448	6.768614	-0.033825	3.455430
169.362787	4021.533691	6.773619	-0.033844	3.458697
169.904164	4029.565243	6.778624	-0.033950	3.461992
169.768637	4037.598317	6.783629	-0.033930	3.465262
170.001624	4045.636362	6.788634	-0.033979	3.468543
170.296846	4053.689463	6.793638	-0.034039	3.471830
170.489364	4061.725452	6.798643	-0.034080	3.475102
170.627556	4069.702657	6.803648	-0.034111	3.478347
170.792937	4077.722184	6.808653	-0.034147	3.481606
170.950025	4085.719909	6.813658	-0.034181	3.484852
171.212944	4093.761587	6.818662	-0.034235	3.488117
171.414511	4101.787176	6.823667	-0.034278	3.491371
171.752965	4109.831278	6.828672	-0.034346	3.494633
171.803973	4117.829692	6.833677	-0.034360	3.497865
171.844066	4125.866575	6.838682	-0.034373	3.501108
172.075710	4133.854220	6.843686	-0.034421	3.504335
172.339927	4141.877066	6.848691	-0.034476	3.507574
172.748420	4149.932798	6.853696	-0.034557	3.510828
173.115410	4157.952774	6.858701	-0.034630	3.514063
173.300842	4165.958494	6.863706	-0.034670	3.517284
173.188080	4174.044330	6.868710	-0.034654	3.520524
173.497834	4181.979805	6.873715	-0.034717	3.523715
173.630518	4190.052337	6.878720	-0.034747	3.526952
173.762687	4198.069939	6.883725	-0.034776	3.530164
173.693033	4206.148515	6.888730	-0.034769	3.533391
174.309104	4214.164555	6.893734	-0.034888	3.536611
174.321104	4222.181353	6.898739	-0.034896	3.539810
174.596398	4230.198123	6.903744	-0.034952	3.543014
174.644243	4238.239367	6.908749	-0.034966	3.546218
174.966471	4246.237528	6.913754	-0.035031	3.549410
175.110272	4254.389937	6.918758	-0.035063	3.552656
175.086886	4262.408206	6.923763	-0.035064	3.555840
175.582615	4270.345484	6.928768	-0.035161	3.559004
175.717635	4278.356978	6.933773	-0.035192	3.562185
175.603928	4286.375957	6.938778	-0.035176	3.565358
175.772801	4294.389876	6.943782	-0.035212	3.568535
176.020480	4302.410751	6.948787	-0.035263	3.571713
176.094643	4310.477710	6.953792	-0.035282	3.574903
176.200906	4318.468061	6.958797	-0.035307	3.578060
176.618011	4326.495904	6.963802	-0.035390	3.581237
176.694379	4334.501969	6.968806	-0.035409	3.584394
176.953520	4342.504246	6.973811	-0.035463	3.587552
177.236449	4350.543739	6.978816	-0.035521	3.590722
177.503259	4358.600380	6.983821	-0.035575	3.593895
177.591962	4366.615042	6.988826	-0.035597	3.597044
177.828300	4374.612637	6.993830	-0.035646	3.600188
178.160886	4382.592912	6.998835	-0.035713	3.603325
178.243082	4390.673955	7.003840	-0.035734	3.606492
178.449347	4398.667087	7.008845	-0.035777	3.609625
178.637018	4406.706938	7.013850	-0.035817	3.612773
179.103565	4414.744537	7.018854	-0.035909	3.615925
178.992892	4422.750094	7.023859	-0.035894	3.619045
179.354988	4430.768472	7.028864	-0.035966	3.622182
179.525029	4438.800243	7.033869	-0.036003	3.625315
179.520258	4446.818388	7.038874	-0.036007	3.628435
180.002067	4454.915475	7.043878	-0.036102	3.631597
180.001143	4462.923234	7.048883	-0.036107	3.634708
180.510581	4470.907235	7.053888	-0.036207	3.637821
180.513335	4478.964816	7.058893	-0.036213	3.640946
180.713139	4486.939952	7.063898	-0.036255	3.644042
180.974869	4495.014504	7.068902	-0.036309	3.647175
181.162217	4502.985775	7.073907	-0.036349	3.650264
181.536111	4511.039192	7.078912	-0.036424	3.653386
181.768850	4519.065641	7.083917	-0.036472	3.656492
181.840647	4527.067893	7.088922	-0.036491	3.659582
182.178306	4535.110741	7.093926	-0.036559	3.662691
182.305133	4543.123775	7.098931	-0.036587	3.665781
182.449561	4551.164357	7.103936	-0.036619	3.668879
182.550768	4559.240707	7.108941	-0.036643	3.671987
182.584174	4567.245587	7.113946	-0.036655	3.675064
182.886157	4575.234337	7.118950	-0.036716	3.678138
182.955609	4583.247875	7.123955	-0.036734	3.681214
183.160889	4591.245258	7.128960	-0.036777	3.684284
183.440572	4599.299122	7.133965	-0.036835	3.687375
183.526438	4607.323718	7.138970	-0.036856	3.690448
183.783392	4615.366637	7.143974	-0.036909	3.693529
183.859728	4623.374303	7.148979	-0.036928	3.696589
184.174698	4631.376271	7.153984	-0.036992	3.699651
184.275526	4639.392463	7.158989	-0.037016	3.702710
184.399751	4647.408072	7.163994	-0.037044	3.705767
184.547191	4655.460029	7.168998	-0.037077	3.708836
184.703785	4663.509103	7.174003	-0.037111	3.711902
184.938515	4671.584514	7.179008	-0.037160	3.714977
185.129975	4679.563413	7.184013	-0.037200	3.718011
185.210975	4687.537081	7.189018	-0.037221	3.721039
185.347318	4695.559878	7.194022	-0.037251	3.724083
185.578993	4703.538699	7.199027	-0.037299	3.727111
185.599558	4711.601089	7.204032	-0.037308	3.730164
185.673201	4719.644434	7.209037	-0.037327	3.733207
185.664588	4727.667349	7.214042	-0.037331	3.736239
186.193792	4735.628961	7.219046	-0.037434	3.739257
186.166085	4743.684404	7.224051	-0.037434	3.742296
186.355974	4751.692984	7.229056	-0.037475	3.745319
186.858717	4759.688585	7.234061	-0.037574	3.748342
186.868319	4767.773029	7.239066	-0.037580	3.751385
187.185709	4775.798431	7.244070	-0.037645	3.754410
186.999199	4783.824225	7.249075	-0.037615	3.757421
187.397086	4791.837806	7.254080	-0.037694	3.760439
187.584869	4799.834290	7.259085	-0.037734	3.763443
187.689639	4807.880671	7.264090	-0.037759	3.766461
188.154859	4815.885684	7.269094	-0.037851	3.769470
188.193862	4823.945796	7.274099	-0.037863	3.772487
188.494943	4831.963899	7.279104	-0.037924	3.775492
188.640388	4839.994602	7.284109	-0.037957	3.778496
188.773223	4848.001571	7.289114	-0.037986	3.781488
188.855774	4856.026344	7.294118	-0.038007	3.784483
188.905951	4864.045211	7.299123	-0.038021	3.787473
189.122621	4872.085657	7.304128	-0.038067	3.790472
189.233036	4880.132185	7.309133	-0.038093	3.793469
189.233875	4888.171475	7.314138	-0.038098	3.796459
189.699082	4896.098015	7.319142	-0.038190	3.799414
189.994598	4904.093098	7.324147	-0.038250	3.802389
190.051964	4912.131303	7.329152	-0.038265	3.805372
190.325609	4920.169922	7.334157	-0.038322	3.808357
190.454971	4928.199785	7.339162	-0.038351	3.811334
190.678110	4936.229690	7.344166	-0.038397	3.814311
190.744028	4944.249750	7.349171	-0.038415	3.817278
191.081074	4952.235905	7.354176	-0.038483	3.820236
191.230798	4960.252725	7.359181	-0.038516	3.823199
191.231892	4968.279289	7.364186	-0.038521	3.826160
191.571507	4976.328297	7.369190	-0.038589	3.829134
191.567482	4984.354131	7.374195	-0.038594	3.832091
191.828106	4992.396588	7.379200	-0.038647	3.835056
192.150698	5000.384136	7.384205	-0.038713	3.838001
192.179760	5008.369030	7.389210	-0.038723	3.840936
192.301347	5016.408430	7.394214	-0.038751	3.843890
192.471530	5024.403687	7.399219	-0.038788	3.846827
193.025758	5032.442465	7.404224	-0.038896	3.849786
192.984112	5040.520833	7.409229	-0.038893	3.852745
193.043573	5048.525569	7.414234	-0.038910	3.855676
193.383451	5056.548257	7.419238	-0.038978	3.858618
193.534931	5064.538890	7.424243	-0.039011	3.861542
193.767683	5072.565395	7.429248	-0.039060	3.864478
193.923172	5080.608327	7.434253	-0.039094	3.867416
194.196903	5088.626173	7.439258	-0.039150	3.870346
194.420179	5096.893798	7.444262	-0.039197	3.873363
194.363834	5104.886314	7.449267	-0.039191	3.876272
194.674587	5112.764603	7.454272	-0.039254	3.879145
194.812076	5120.774143	7.459277	-0.039285	3.882059
194.983455	5128.734655	7.464282	-0.039322	3.884955
195.506101	5136.765912	7.469286	-0.039424	3.887880
195.638432	5144.767356	7.474291	-0.039454	3.890785
195.890775	5152.836562	7.479296	-0.039506	3.893715
196.157195	5160.869829	7.484301	-0.039561	3.896630
196.315826	5168.812204	7.489306	-0.039596	3.899507
196.515872	5176.868028	7.494310	-0.039638	3.902424
196.675835	5184.863788	7.499315	-0.039673	3.905317
196.899352	5192.883007	7.504320	-0.039720	3.908217
197.156427	5200.929052	7.509325	-0.039773	3.911125
196.955365	5208.943323	7.514330	-0.039740	3.914011
197.234169	5216.997728	7.519334	-0.039797	3.916918
197.309457	5224.945478	7.524339	-0.039817	3.919781
197.403731	5232.992730	7.529344	-0.039839	3.922678
197.575608	5240.986440	7.534349	-0.039876	3.925555
197.638792	5248.990722	7.539354	-0.039893	3.928432
198.007454	5257.034233	7.544358	-0.039967	3.931326
198.028328	5265.056889	7.549363	-0.039976	3.934204
198.123996	5273.128746	7.554368	-0.039999	3.937099
198.353958	5281.117941	7.559373	-0.040047	3.939965
198.439883	5289.110605	7.564378	-0.040068	3.942827
198.589013	5297.140051	7.569382	-0.040101	3.945701
198.806459	5305.142350	7.574387	-0.040147	3.948565
198.998515	5313.186782	7.579392	-0.040187	3.951441
199.261075	5321.245099	7.584397	-0.040241	3.954322
199.444961	5329.239671	7.589402	-0.040281	3.957176
199.449803	5337.258413	7.594406	-0.040287	3.960033
199.463590	5345.236041	7.599411	-0.040294	3.962874
199.775796	5353.268259	7.604416	-0.040358	3.965738
200.103707	5361.259119	7.609421	-0.040424	3.968585
200.170096	5369.298213	7.614426	-0.040441	3.971443
200.390662	5377.389470	7.619430	-0.040488	3.974319
200.498878	5385.379330	7.624435	-0.040513	3.977156
200.645442	5393.389878	7.629440	-0.040545	3.979998
200.871231	5401.384877	7.634445	-0.040592	3.982835
200.968480	5409.394326	7.639450	-0.040616	3.985672
201.392030	5417.444676	7.644454	-0.040700	3.988527
201.516540	5425.457405	7.649459	-0.040728	3.991362
201.639011	5433.517534	7.654464	-0.040756	3.994211
201.831821	5441.556362	7.659469	-0.040797	3.997052
201.845217	5449.522441	7.664474	-0.040805	3.999863
201.995237	5457.578279	7.669478	-0.040838	4.002705
202.371984	5465.546301	7.674483	-0.040913	4.005518
202.300542	5473.600646	7.679488	-0.040905	4.008352
202.410940	5481.644506	7.684493	-0.040930	4.011183
202.518979	5489.658671	7.689498	-0.040956	4.014002
202.829134	5497.707748	7.694502	-0.041019	4.016835
202.792292	5505.678388	7.699507	-0.041017	4.019632
203.042333	5513.697993	7.704512	-0.041068	4.022449
203.274547	5521.740153	7.709517	-0.041117	4.025271
203.295461	5529.762539	7.714522	-0.041126	4.028082
203.551848	5537.754409	7.719526	-0.041179	4.030883
203.959036	5545.868623	7.724531	-0.041260	4.033728
204.230052	5553.887408	7.729536	-0.041315	4.036535
204.104796	5561.837732	7.734541	-0.041297	4.039310
204.006155	5569.848707	7.739546	-0.041284	4.042105
204.458412	5577.837244	7.744550	-0.041373	4.044898
204.499481	5585.868649	7.749555	-0.041386	4.047698
204.816320	5593.849169	7.754560	-0.041450	4.050483
205.049014	5601.918707	7.759565	-0.041498	4.053295
205.098468	5609.949544	7.764570	-0.041513	4.056089
205.232659	5617.928511	7.769574	-0.041543	4.058865
205.188464	5625.978834	7.774579	-0.041540	4.061660
205.626710	5633.928425	7.779584	-0.041626	4.064426
205.570488	5642.005652	7.784589	-0.041621	4.067227
205.737816	5649.989205	7.789594	-0.041657	4.069997
206.072591	5658.055310	7.794598	-0.041725	4.072796
206.177804	5666.046181	7.799603	-0.041750	4.075563
206.273574	5674.036595	7.804608	-0.041772	4.078329
206.435874	5682.083115	7.809613	-0.041808	4.081113
206.525444	5690.052221	7.814618	-0.041830	4.083867
206.769035	5698.140957	7.819622	-0.041880	4.086663
206.918356	5706.119568	7.824627	-0.041913	4.089417
207.278361	5714.151513	7.829632	-0.041985	4.092191
207.406175	5722.174574	7.834637	-0.042014	4.094957
207.492227	5730.175717	7.839642	-0.042035	4.097713
207.770284	5738.230228	7.844646	-0.042092	4.100488
207.838914	5746.193923	7.849651	-0.042110	4.103227
207.873338	5754.248819	7.854656	-0.042122	4.105995
208.188818	5762.284813	7.859661	-0.042185	4.108758
208.371778	5770.289512	7.864666	-0.042225	4.111507
208.791365	5778.338083	7.869670	-0.042308	4.114272
208.891188	5786.349570	7.874675	-0.042332	4.117018
209.021670	5794.328827	7.879680	-0.042361	4.119752
209.082606	5802.368964	7.884685	-0.042377	4.122504
209.235873	5810.327986	7.889690	-0.042411	4.125228
209.516309	5818.379964	7.894694	-0.042468	4.127983
209.624072	5826.431871	7.899699	-0.042494	4.130734
209.830820	5834.496579	7.904704	-0.042537	4.133489
209.837744	5842.515384	7.909709	-0.042544	4.136224
209.812631	5850.461855	7.914714	-0.042544	4.138932
209.990502	5858.562139	7.919718	-0.042582	4.141693
210.103684	5866.514230	7.924723	-0.042609	4.144401
210.575928	5874.570878	7.929728	-0.042702	4.147147
210.545992	5882.578166	7.934733	-0.042701	4.149869
210.539415	5890.636776	7.939738	-0.042705	4.152606
210.899599	5898.651138	7.944742	-0.042777	4.155331
211.026430	5906.614556	7.949747	-0.042806	4.158034
211.081890	5914.643706	7.954752	-0.042821	4.160757
211.269841	5922.670844	7.959757	-0.042862	4.163478
211.448352	5930.670434	7.964762	-0.042900	4.166189
211.716481	5938.679665	7.969766	-0.042955	4.168902
211.682329	5946.738577	7.974771	-0.042954	4.171627
211.954622	5954.744439	7.979776	-0.043010	4.174335
211.961984	5962.783852	7.984781	-0.043016	4.177050
212.029046	5970.780261	7.989786	-0.043034	4.179749
212.508717	5978.825723	7.994790	-0.043128	4.182468
212.551855	5986.801006	7.999795	-0.043141	4.185156
212.671465	5994.829028	8.004800	-0.043169	4.187861
212.995376	6002.802814	8.009805	-0.043234	4.190549
213.112557	6010.951899	8.014810	-0.043261	4.193291
213.208917	6018.998339	8.019814	-0.043284	4.195997
213.163784	6026.878803	8.024819	-0.043281	4.198644
213.465093	6034.929125	8.029824	-0.043342	4.201350
213.564164	6042.889639	8.034829	-0.043366	4.204021
213.382721	6050.919882	8.039834	-0.043337	4.206712
213.701801	6058.922941	8.044838	-0.043401	4.209397
214.050758	6066.948982	8.049843	-0.043471	4.212088
214.310537	6074.989563	8.054848	-0.043525	4.214781
214.532499	6083.000127	8.059853	-0.043571	4.217463
214.600449	6090.985956	8.064858	-0.043589	4.220132
214.841096	6099.017521	8.069862	-0.043639	4.222817
214.902365	6107.040928	8.074867	-0.043656	4.225496
214.994550	6115.071353	8.079872	-0.043678	4.228175
215.109423	6123.094072	8.084877	-0.043704	4.230851
215.206492	6131.106507	8.089882	-0.043728	4.233521
215.464472	6139.163471	8.094886	-0.043781	4.236206
215.588167	6147.128154	8.099891	-0.043809	4.238857
215.822016	6155.185834	8.104896	-0.043858	4.241539
215.730747	6163.160209	8.109901	-0.043846	4.244188
215.854559	6171.181429	8.114906	-0.043874	4.246853
215.964368	6179.221312	8.119910	-0.043899	4.249522
215.922977	6187.263917	8.124915	-0.043897	4.252189
216.350156	6195.273180	8.129920	-0.043982	4.254848
216.797491	6203.287082	8.134925	-0.044070	4.257507
216.528026	6211.282305	8.139930	-0.044025	4.260151
216.744289	6219.334395	8.144934	-0.044070	4.262817
217.088395	6227.335295	8.149939	-0.044140	4.265465
217.318962	6235.365132	8.154944	-0.044188	4.268121
217.177096	6243.424108	8.159949	-0.044166	4.270780
217.246081	6251.428581	8.164954	-0.044184	4.273423
217.460296	6259.496755	8.169958	-0.044229	4.276085
217.595476	6267.413862	8.174963	-0.044260	4.278696
217.671825	6275.492864	8.179968	-0.044279	4.281358
217.689078	6283.457006	8.184973	-0.044287	4.283980
217.777493	6291.479299	8.189978	-0.044309	4.286620
217.945779	6299.511225	8.194982	-0.044345	4.289262
218.264069	6307.530188	8.199987	-0.044410	4.291899
218.464226	6315.565698	8.204992	-0.044452	4.294540
218.446970	6323.576358	8.209997	-0.044454	4.297168
218.658160	6331.535903	8.215002	-0.044498	4.299780
218.923079	6339.571496	8.220006	-0.044553	4.302416
218.697640	6347.570475	8.225011	-0.044516	4.305035
219.087009	6355.618795	8.230016	-0.044594	4.307673
219.407610	6363.621331	8.235021	-0.044658	4.310293
219.428806	6371.701768	8.240026	-0.044667	4.312935
219.509384	6379.732280	8.245030	-0.044688	4.315560
219.467327	6387.688292	8.250035	-0.044685	4.318158
219.833938	6395.711553	8.255040	-0.044758	4.320779
220.012566	6403.723017	8.260045	-0.044797	4.323393
220.096164	6411.729081	8.265050	-0.044817	4.326004
220.331532	6419.764456	8.270054	-0.044866	4.328623
220.370999	6427.759227	8.275059	-0.044879	4.331226
220.348727	6435.811045	8.280064	-0.044880	4.333846
220.538862	6443.842979	8.285069	-0.044920	4.336459
220.375813	6451.778810	8.290074	-0.044895	4.339037
220.764757	6459.828752	8.295078	-0.044973	4.341654
220.903756	6467.814881	8.300083	-0.045004	4.344247
220.874003	6475.870971	8.305088	-0.045003	4.346860
221.020849	6483.920557	8.310093	-0.045036	4.349471
221.126406	6491.940226	8.315098	-0.045060	4.352070
221.353064	6500.016298	8.320102	-0.045108	4.354686
221.562906	6507.994404	8.325107	-0.045152	4.357270
221.686164	6515.926910	8.330112	-0.045180	4.359836
221.968104	6523.972140	8.335117	-0.045238	4.362438
221.986024	6531.910451	8.340122	-0.045246	4.365003
222.067461	6540.017636	8.345126	-0.045266	4.367620
222.255971	6547.982496	8.350131	-0.045306	4.370191
222.418863	6556.035903	8.355136	-0.045342	4.372789
222.378572	6564.056295	8.360141	-0.045340	4.375373
222.299371	6572.048202	8.365146	-0.045330	4.377947
222.660461	6580.069724	8.370150	-0.045402	4.380531
222.824721	6588.084162	8.375155	-0.045438	4.383110
222.855021	6596.070822	8.380160	-0.045449	4.385678
223.086093	6604.150962	8.385165	-0.045497	4.388275
223.179091	6612.150880	8.390170	-0.045519	4.390845
223.565495	6620.185481	8.395174	-0.045596	4.393426
223.679695	6628.220864	8.400179	-0.045623	4.396003
224.172255	6636.180570	8.405184	-0.045720	4.398557
224.673494	6644.227824	8.410189	-0.045818	4.401138
225.058388	6652.147323	8.415194	-0.045895	4.403676
225.394367	6660.209964	8.420198	-0.045963	4.406257
225.378557	6668.256785	8.425203	-0.045965	4.408830
225.523766	6676.294993	8.430208	-0.045997	4.411400
225.859341	6684.345710	8.435213	-0.046065	4.413973
225.839971	6692.339284	8.440218	-0.046066	4.416525
225.951993	6700.338400	8.445222	-0.046092	4.419077
225.978533	6708.396377	8.450227	-0.046102	4.421647
226.339625	6716.342332	8.455232	-0.046174	4.424181
226.341264	6724.441466	8.460237	-0.046180	4.426760
226.293372	6732.402808	8.465242	-0.046176	4.429294
226.631709	6740.487817	8.470246	-0.046244	4.431867
226.784253	6748.526279	8.475251	-0.046278	4.434424
226.923735	6756.516557	8.480256	-0.046309	4.436963
227.141763	6764.513340	8.485261	-0.046354	4.439503
227.185585	6772.514217	8.490266	-0.046368	4.442043
227.381490	6780.469413	8.495270	-0.046409	4.444567
227.639780	6788.542666	8.500275	-0.046463	4.447127
227.872607	6796.525401	8.505280	-0.046511	4.449657
227.922032	6804.601923	8.510285	-0.046525	4.452215
227.874949	6812.586638	8.515290	-0.046522	4.454742
228.077715	6820.625100	8.520294	-0.046565	4.457285
228.212435	6828.598929	8.525299	-0.046595	4.459806
228.194631	6836.616731	8.530304	-0.046597	4.462339
228.486845	6844.653218	8.535309	-0.046656	4.464877
228.641445	6852.650482	8.540314	-0.046690	4.467401
228.681509	6860.721975	8.545318	-0.046703	4.469947
228.572875	6868.732397	8.550323	-0.046688	4.472472
228.888231	6876.713863	8.555328	-0.046751	4.474987
229.049957	6884.741299	8.560333	-0.046787	4.477515
229.158694	6892.713370	8.565338	-0.046812	4.480024
229.251333	6900.778508	8.570343	-0.046834	4.482560
229.544488	6908.740872	8.575347	-0.046894	4.485064
229.643023	6916.813167	8.580352	-0.046917	4.487600
229.603445	6924.801918	8.585357	-0.046915	4.490108
229.736531	6932.808379	8.590362	-0.046945	4.492620
229.914734	6940.858787	8.595367	-0.046983	4.495145
229.961039	6948.876169	8.600371	-0.046997	4.497658
230.094412	6956.860378	8.605376	-0.047027	4.500160
230.301139	6964.897311	8.610381	-0.047071	4.502676
230.244172	6972.884246	8.615386	-0.047065	4.505175
230.493259	6980.936896	8.620391	-0.047117	4.507694
230.655779	6988.946917	8.625395	-0.047152	4.510198
230.664355	6997.002707	8.630400	-0.047159	4.512714
230.908062	7005.043127	8.635405	-0.047209	4.515225
231.163219	7013.000959	8.640410	-0.047262	4.517708
231.210671	7020.989887	8.645415	-0.047276	4.520200
231.228144	7028.966436	8.650419	-0.047284	4.522686
231.328758	7036.968846	8.655424	-0.047308	4.525179
231.685782	7045.029094	8.660429	-0.047380	4.527689
231.675647	7052.989066	8.665434	-0.047383	4.530166
231.722567	7061.092608	8.670439	-0.047397	4.532686
231.789858	7069.102087	8.675443	-0.047414	4.535175
231.887963	7077.102739	8.680448	-0.047438	4.537661
231.965631	7085.119012	8.685453	-0.047457	4.540149
232.191258	7093.085518	8.690458	-0.047505	4.542622
232.372548	7101.122163	8.695463	-0.047543	4.545114
232.521742	7109.137278	8.700467	-0.047576	4.547599
232.553686	7117.185683	8.705472	-0.047587	4.550092
232.557353	7125.236649	8.710477	-0.047593	4.552585
232.693011	7133.241943	8.715482	-0.047624	4.555062
233.012908	7141.250798	8.720487	-0.047688	4.557539
233.087140	7149.193506	8.725491	-0.047707	4.559994
233.243024	7157.265531	8.730496	-0.047741	4.562488
233.414393	7165.254995	8.735501	-0.047778	4.564955
233.426769	7173.287928	8.740506	-0.047786	4.567434
233.615384	7181.274973	8.745511	-0.047826	4.569898
233.831228	7189.364584	8.750515	-0.047871	4.572392
234.127568	7197.322609	8.755520	-0.047932	4.574844
234.374760	7205.392685	8.760525	-0.047983	4.577329
234.273745	7213.344463	8.765530	-0.047969	4.579776
234.457771	7221.355530	8.770535	-0.048008	4.582240
234.445970	7229.379608	8.775539	-0.048011	4.584707
234.806754	7237.488457	8.780544	-0.048084	4.587198
234.680793	7245.471713	8.785549	-0.048065	4.589650
234.795012	7253.449573	8.790554	-0.048092	4.592098
235.265504	7261.523766	8.795559	-0.048185	4.594575
235.204603	7269.549342	8.800563	-0.048178	4.597036
235.292312	7277.496450	8.805568	-0.048200	4.599471
235.659133	7285.571891	8.810573	-0.048273	4.601944
235.892227	7293.478513	8.815578	-0.048322	4.604364
236.096070	7301.560909	8.820583	-0.048365	4.606837
236.235098	7309.553807	8.825587	-0.048396	4.609281
236.282899	7317.615423	8.830592	-0.048410	4.611744
236.296528	7325.679336	8.835597	-0.048417	4.614207
236.312566	7333.594124	8.840602	-0.048425	4.616623
236.726097	7341.610387	8.845607	-0.048508	4.619069
236.655055	7349.673885	8.850611	-0.048500	4.621528
236.818225	7357.610645	8.855616	-0.048535	4.623947
236.880728	7365.715579	8.860621	-0.048552	4.626416
237.010045	7373.653645	8.865626	-0.048581	4.628833
237.515809	7381.732854	8.870631	-0.048680	4.631291
237.422026	7389.759261	8.875635	-0.048668	4.633732
237.540187	7397.793286	8.880640	-0.048695	4.636174
237.695929	7405.734017	8.885645	-0.048729	4.638586
237.978885	7413.758387	8.890650	-0.048787	4.641023
238.144887	7421.746710	8.895655	-0.048823	4.643447
238.086653	7429.803613	8.900659	-0.048817	4.645891
238.294098	7437.807735	8.905664	-0.048861	4.648317
238.654401	7445.851586	8.910669	-0.048933	4.650754
238.431807	7453.853755	8.915674	-0.048897	4.653178
238.514467	7461.925969	8.920679	-0.048917	4.655621
238.977586	7469.891212	8.925683	-0.049009	4.658031
238.831848	7477.881347	8.930688	-0.048987	4.660447
238.723950	7485.898452	8.935693	-0.048972	4.662870
239.100779	7493.884366	8.940698	-0.049047	4.665281
239.356613	7501.933031	8.945703	-0.049100	4.667711
239.292392	7509.926666	8.950707	-0.049093	4.670123
239.244094	7518.041497	8.955712	-0.049089	4.672570
239.604274	7526.135547	8.960717	-0.049161	4.675010
239.657164	7534.053147	8.965722	-0.049176	4.677395
239.854183	7542.011845	8.970727	-0.049218	4.679791
240.018797	7550.052357	8.975731	-0.049254	4.682210
240.303824	7557.956565	8.980736	-0.049312	4.684588
240.579618	7566.036240	8.985741	-0.049368	4.687016
240.356038	7574.013373	8.990746	-0.049332	4.689414
240.527954	7582.175745	8.995751	-0.049369	4.691865
240.768545	7590.110892	9.000755	-0.049419	4.694246
240.667138	7598.107298	9.005760	-0.049405	4.696645
241.031363	7606.101475	9.010765	-0.049478	4.699042
241.130296	7614.157462	9.015770	-0.049502	4.701456
241.205106	7622.106962	9.020775	-0.049521	4.703837
241.254916	7630.170907	9.025779	-0.049535	4.706251
241.485859	7638.138092	9.030784	-0.049583	4.708635
241.604895	7646.221322	9.035789	-0.049611	4.711052
241.667035	7654.265484	9.040794	-0.049627	4.713457
241.831128	7662.305194	9.045799	-0.049663	4.715859
241.658093	7670.212464	9.050803	-0.049636	4.718221
241.803941	7678.240348	9.055808	-0.049668	4.720616
242.078604	7686.291272	9.060813	-0.049724	4.723018
242.365993	7694.261688	9.065818	-0.049783	4.725393
242.495713	7702.376277	9.070823	-0.049812	4.727811
242.453722	7710.343589	9.075827	-0.049810	4.730185
242.711901	7718.373293	9.080832	-0.049863	4.732575
242.815827	7726.447667	9.085837	-0.049887	4.734977
242.868835	7734.398647	9.090842	-0.049902	4.737342
243.271791	7742.382316	9.095847	-0.049982	4.739714
243.552104	7750.398334	9.100851	-0.050040	4.742095
243.699499	7758.358235	9.105856	-0.050072	4.744458
243.911834	7766.492240	9.110861	-0.050117	4.746872
243.836123	7774.445282	9.115866	-0.050108	4.749231
244.046834	7782.519124	9.120871	-0.050152	4.751624
244.295893	7790.572263	9.125875	-0.050204	4.754010
244.262149	7798.526202	9.130880	-0.050203	4.756366
244.693645	7806.544276	9.135885	-0.050288	4.758739
244.663675	7814.512585	9.140890	-0.050288	4.761097
244.770210	7822.522361	9.145895	-0.050313	4.763466
245.050438	7830.562567	9.150899	-0.050370	4.765841
244.985269	7838.512825	9.155904	-0.050363	4.768191
245.058165	7846.612516	9.160909	-0.050382	4.770583
245.334774	7854.594049	9.165914	-0.050438	4.772937
245.636270	7862.665695	9.170919	-0.050499	4.775318
245.650193	7870.638191	9.175923	-0.050507	4.777669
245.716793	7878.628038	9.180928	-0.050525	4.780023
245.993707	7886.694649	9.185933	-0.050581	4.782398
245.820181	7894.637275	9.190938	-0.050554	4.784738
245.973812	7902.686936	9.195943	-0.050588	4.787106
246.218874	7910.669741	9.200947	-0.050639	4.789453
246.377179	7918.798721	9.205952	-0.050673	4.791842
246.641639	7926.755888	9.210957	-0.050728	4.794180
246.626055	7934.783127	9.215962	-0.050730	4.796537
246.627880	7942.739049	9.220967	-0.050735	4.798873
246.692619	7950.781747	9.225971	-0.050752	4.801232
246.892727	7958.726141	9.230976	-0.050795	4.803561
247.127229	7966.859303	9.235981	-0.050844	4.805945
246.983509	7974.826566	9.240986	-0.050822	4.808279
247.213898	7982.854742	9.245991	-0.050870	4.810629
247.356479	7990.416109	9.250995	-0.050901	4.812842
247.407520	7995.119267	9.256000	-0.050914	4.814218

247.562548	7997.739741	9.261005	-0.050944	4.814984
247.542909	7999.058707	9.266010	-0.050941	4.815370
247.725092	7999.534524	9.271015	-0.050975	4.815508
247.675387	8000.438946	9.276019	-0.050967	4.815773
247.845135	8000.575130	9.281024	-0.050998	4.815812
248.008113	8000.475278	9.286029	-0.051028	4.815782
247.918366	8000.574163	9.291034	-0.051012	4.815811
248.076213	8000.480634	9.296039	-0.051041	4.815783
248.195723	8000.569033	9.301043	-0.051063	4.815808
248.192875	8000.586058	9.306048	-0.051062	4.815813
248.378733	8000.498321	9.311053	-0.051097	4.815787
248.280874	8000.572521	9.316058	-0.051079	4.815809
248.425570	8000.590871	9.321063	-0.051106	4.815813
248.327260	8000.486783	9.326067	-0.051087	4.815784
248.281652	8000.587452	9.331072	-0.051079	4.815813
248.572207	8000.489668	9.336077	-0.051132	4.815783
248.388227	8000.573148	9.341082	-0.051098	4.815808
248.610470	8000.502013	9.346087	-0.051139	4.815787
248.573333	8000.480051	9.351091	-0.051132	4.815780
248.339007	8000.576593	9.356096	-0.051089	4.815810
248.414890	8000.397399	9.361101	-0.051103	4.815757
248.536819	8000.580849	9.366106	-0.051125	4.815810
248.937701	8000.586272	9.371111	-0.051200	4.815810
248.691798	8000.457372	9.376115	-0.051154	4.815773
248.701218	8000.584555	9.381120	-0.051156	4.815810
248.781822	8000.591190	9.386125	-0.051170	4.815812
248.966068	8000.492750	9.391130	-0.051205	4.815782
248.970132	8000.496010	9.396135	-0.051205	4.815783
248.763270	8000.402972	9.401139	-0.051167	4.815757
248.873270	8000.371652	9.406144	-0.051187	4.815747
248.827909	8000.513960	9.411149	-0.051178	4.815789
248.758310	8000.417810	9.416154	-0.051165	4.815761
249.014718	8000.473200	9.421159	-0.051213	4.815776
248.804772	8000.490071	9.426163	-0.051174	4.815782
248.853417	8000.593336	9.431168	-0.051183	4.815812
248.992753	8000.503776	9.436173	-0.051209	4.815785
248.915020	8000.568695	9.441178	-0.051194	4.815805
248.885181	8000.490270	9.446183	-0.051188	4.815782
249.025379	8000.498940	9.451187	-0.051214	4.815784
249.205138	8000.604332	9.456192	-0.051248	4.815814
249.122700	8000.494094	9.461197	-0.051232	4.815782
249.227806	8000.566249	9.466202	-0.051252	4.815803
249.374100	8000.532315	9.471207	-0.051279	4.815792
249.335597	8000.376884	9.476211	-0.051272	4.815747
249.189360	8000.605098	9.481216	-0.051244	4.815814
249.280224	8000.404792	9.486221	-0.051261	4.815755
249.370739	8000.596278	9.491226	-0.051278	4.815811
249.347740	8000.434693	9.496231	-0.051273	4.815764
249.254244	8000.497221	9.501235	-0.051256	4.815782
249.363458	8000.398632	9.506240	-0.051276	4.815753
249.465424	8000.492087	9.511245	-0.051295	4.815780
249.245928	8000.505600	9.516250	-0.051254	4.815785
249.237668	8000.377349	9.521255	-0.051252	4.815747
249.372998	8000.594115	9.526259	-0.051278	4.815810
249.470517	8000.498539	9.531264	-0.051296	4.815782
249.388666	8000.489729	9.536269	-0.051280	4.815779
249.313353	8000.387080	9.541274	-0.051266	4.815750
249.262667	8000.486600	9.546279	-0.051257	4.815779
249.384440	8000.392485	9.551283	-0.051279	4.815751
249.439330	8000.485176	9.556288	-0.051289	4.815778
249.381644	8000.406299	9.561293	-0.051278	4.815755
249.491701	8000.396331	9.566298	-0.051299	4.815752
249.595799	8000.374524	9.571303	-0.051318	4.815745
249.350282	8000.397223	9.576307	-0.051272	4.815753
249.370847	8000.461601	9.581312	-0.051276	4.815771
249.595421	8000.390504	9.586317	-0.051318	4.815749
249.658111	8000.597553	9.591322	-0.051329	4.815810
249.438419	8000.412494	9.596327	-0.051288	4.815757
249.428329	8000.380294	9.601331	-0.051286	4.815747
249.372542	8000.507488	9.606336	-0.051276	4.815785
249.561222	8000.369620	9.611341	-0.051311	4.815744
249.550201	8000.588284	9.616346	-0.051309	4.815808
249.758880	8000.395225	9.621351	-0.051347	4.815750
249.677240	8000.491041	9.626355	-0.051332	4.815779
249.717661	8000.391336	9.631360	-0.051339	4.815749
249.864692	8000.371292	9.636365	-0.051367	4.815743
249.855749	8000.498180	9.641370	-0.051365	4.815780
249.601545	8000.420385	9.646375	-0.051318	4.815758
249.502049	8000.363249	9.651379	-0.051299	4.815742
249.652509	8000.486315	9.656384	-0.051327	4.815777
249.775690	8000.506453	9.661389	-0.051350	4.815783
249.647334	8000.581227	9.666394	-0.051326	4.815805
249.766315	8000.394187	9.671399	-0.051348	4.815750
249.644031	8000.380451	9.676403	-0.051325	4.815746
249.423488	8000.483623	9.681408	-0.051284	4.815778
249.637695	8000.417695	9.686413	-0.051323	4.815757
249.741933	8000.580581	9.691418	-0.051343	4.815804
249.860612	8000.517374	9.696423	-0.051365	4.815785
249.644124	8000.382542	9.701427	-0.051324	4.815747
249.656781	8000.520455	9.706432	-0.051327	4.815787
249.875289	8000.498368	9.711437	-0.051367	4.815780
250.052712	8000.470277	9.716442	-0.051400	4.815771
250.017350	8000.383220	9.721447	-0.051393	4.815745
250.038517	8000.492448	9.726451	-0.051397	4.815777
249.874199	8000.400097	9.731456	-0.051366	4.815751
249.998932	8000.328448	9.736461	-0.051390	4.815729
249.973249	8000.544741	9.741466	-0.051385	4.815793
249.843061	8000.401699	9.746471	-0.051360	4.815752
249.841385	8000.495610	9.751475	-0.051360	4.815779
249.904141	8000.399469	9.756480	-0.051372	4.815751
249.935282	8000.496047	9.761485	-0.051377	4.815779
249.805843	8000.483263	9.766490	-0.051353	4.815776
249.938186	8000.520630	9.771495	-0.051378	4.815786
249.891693	8000.499583	9.776499	-0.051369	4.815780
249.671397	8000.502406	9.781504	-0.051328	4.815782
249.994201	8000.435037	9.786509	-0.051388	4.815761
250.026569	8000.428080	9.791514	-0.051394	4.815759
250.036198	8000.390862	9.796519	-0.051395	4.815748
249.922616	8000.450930	9.801523	-0.051374	4.815766
249.958018	8000.332994	9.806528	-0.051380	4.815731
250.072622	8000.483237	9.811533	-0.051402	4.815774
250.044363	8000.372809	9.816538	-0.051396	4.815742
250.086595	8000.264592	9.821543	-0.051404	4.815710
249.987010	8000.367590	9.826547	-0.051385	4.815741
249.862257	8000.490464	9.831552	-0.051362	4.815778
249.949051	8000.405389	9.836557	-0.051378	4.815752
249.872507	8000.369976	9.841562	-0.051364	4.815742
250.035167	8000.368334	9.846567	-0.051394	4.815741
249.949169	8000.316754	9.851571	-0.051378	4.815726
250.105199	8000.495426	9.856576	-0.051407	4.815778
250.092709	8000.243266	9.861581	-0.051404	4.815704
249.970030	8000.507094	9.866586	-0.051382	4.815782
250.098757	8000.507038	9.871591	-0.051405	4.815781
250.071153	8000.493770	9.876595	-0.051400	4.815778
250.114665	8000.386641	9.881600	-0.051408	4.815746
250.192699	8000.491453	9.886605	-0.051423	4.815776
250.301288	8000.473989	9.891610	-0.051443	4.815771
250.294799	8000.520848	9.896615	-0.051441	4.815784
250.245133	8000.515763	9.901619	-0.051432	4.815783
250.156362	8000.380866	9.906624	-0.051415	4.815744
250.377022	8000.372692	9.911629	-0.051456	4.815741
250.162934	8000.480239	9.916634	-0.051416	4.815773
250.330130	8000.485077	9.921639	-0.051447	4.815774
250.116198	8000.383380	9.926643	-0.051407	4.815745
250.063738	8000.600308	9.931648	-0.051398	4.815809
250.265179	8000.386846	9.936653	-0.051435	4.815745
250.141504	8000.493724	9.941658	-0.051412	4.815777
250.119158	8000.512569	9.946663	-0.051408	4.815783
250.136669	8000.484019	9.951667	-0.051411	4.815774
250.147982	8000.489532	9.956672	-0.051413	4.815776
250.192130	8000.395223	9.961677	-0.051421	4.815748
250.192187	8000.503041	9.966682	-0.051421	4.815780
250.237492	8000.392738	9.971687	-0.051429	4.815747
250.189432	8000.400490	9.976691	-0.051420	4.815750
250.106639	8000.593439	9.981696	-0.051405	4.815807
250.459412	8000.414459	9.986701	-0.051470	4.815753
250.355519	8000.460806	9.991706	-0.051451	4.815767
250.363591	8000.411819	9.996711	-0.051452	4.815752
250.333521	8000.481783	10.001715	-0.051446	4.815773
250.227944	8000.388249	10.006720	-0.051427	4.815746
250.256333	8000.387633	10.011725	-0.051432	4.815746
250.275461	8000.488287	10.016730	-0.051435	4.815775
250.279447	8000.491545	10.021735	-0.051436	4.815776
250.239905	8000.588045	10.026739	-0.051429	4.815804
250.384701	8000.480423	10.031744	-0.051455	4.815772
250.372116	8000.502629	10.036749	-0.051453	4.815779
250.501210	8000.487633	10.041754	-0.051477	4.815774
250.515842	8000.390710	10.046759	-0.051479	4.815745
250.514266	8000.425906	10.051763	-0.051479	4.815756
250.306489	8000.564516	10.056768	-0.051440	4.815797
250.409041	8000.408167	10.061773	-0.051459	4.815751
250.281443	8000.468008	10.066778	-0.051435	4.815769
250.235285	8000.493940	10.071783	-0.051427	4.815777
250.371455	8000.418206	10.076787	-0.051452	4.815754
250.493547	8000.457543	10.081792	-0.051474	4.815765
250.311374	8000.376644	10.086797	-0.051440	4.815742
250.452782	8000.571096	10.091802	-0.051467	4.815798
250.502933	8000.505709	10.096807	-0.051476	4.815779
250.294245	8000.515125	10.101811	-0.051437	4.815783
250.276012	8000.489198	10.106816	-0.051433	4.815775
250.219202	8000.504281	10.111821	-0.051423	4.815780
250.325921	8000.594614	10.116826	-0.051443	4.815806
250.291819	8000.401885	10.121831	-0.051436	4.815750
250.217102	8000.525572	10.126835	-0.051422	4.815786
250.264971	8000.573313	10.131840	-0.051431	4.815800
250.352966	8000.414593	10.136845	-0.051447	4.815753
250.430201	8000.380606	10.141850	-0.051461	4.815743
250.551627	8000.385769	10.146855	-0.051484	4.815744
250.472052	8000.475215	10.151859	-0.051469	4.815770
250.265812	8000.503887	10.156864	-0.051431	4.815780
250.571944	8000.387139	10.161869	-0.051487	4.815744
250.570010	8000.502399	10.166874	-0.051487	4.815778
250.433613	8000.366728	10.171879	-0.051461	4.815739
250.301709	8000.504433	10.176883	-0.051437	4.815780
250.498810	8000.475594	10.181888	-0.051473	4.815770
250.451523	8000.239949	10.186893	-0.051464	4.815702
250.205719	8000.509254	10.191898	-0.051419	4.815782
250.385915	8000.400071	10.196903	-0.051452	4.815749
250.525982	8000.453578	10.201907	-0.051478	4.815764
250.329532	8000.499492	10.206912	-0.051441	4.815778
250.532224	8000.385336	10.211917	-0.051479	4.815744
250.465632	8000.395990	10.216922	-0.051466	4.815747
250.650031	8000.373350	10.221927	-0.051501	4.815740
250.473846	8000.490053	10.226931	-0.051468	4.815775
250.488079	8000.499883	10.231936	-0.051470	4.815778
250.611398	8000.502942	10.236941	-0.051493	4.815778
250.487603	8000.509465	10.241946	-0.051470	4.815780
250.646699	8000.403142	10.246951	-0.051500	4.815749
250.481937	8000.497611	10.251955	-0.051469	4.815777
250.616397	8000.506189	10.256960	-0.051494	4.815779
250.587209	8000.391474	10.261965	-0.051488	4.815745
250.499229	8000.397511	10.266970	-0.051472	4.815748
250.475431	8000.464374	10.271975	-0.051467	4.815767
250.576277	8000.391269	10.276979	-0.051486	4.815745
250.736501	8000.486740	10.281984	-0.051516	4.815773
250.771631	8000.506518	10.286989	-0.051522	4.815778
250.616137	8000.400429	10.291994	-0.051493	4.815748
250.653505	8000.402093	10.296999	-0.051500	4.815748
250.627559	8000.476395	10.302003	-0.051495	4.815770
250.685577	8000.416474	10.307008	-0.051505	4.815752
250.707429	8000.479808	10.312013	-0.051509	4.815771
250.561543	8000.495581	10.317018	-0.051482	4.815776
250.711550	8000.516155	10.322023	-0.051510	4.815781
250.639979	8000.377264	10.327027	-0.051497	4.815741
250.612147	8000.496374	10.332032	-0.051491	4.815776
250.677208	8000.400270	10.337037	-0.051503	4.815748
250.699431	8000.492434	10.342042	-0.051507	4.815774
250.616349	8000.498550	10.347047	-0.051492	4.815777
250.788930	8000.409528	10.352051	-0.051524	4.815750
250.601383	8000.501492	10.357056	-0.051489	4.815778
250.709815	8000.476552	10.362061	-0.051509	4.815770
250.742991	8000.478149	10.367066	-0.051515	4.815770
250.928948	8000.497171	10.372071	-0.051549	4.815775
250.668188	8000.488660	10.377075	-0.051501	4.815774
250.654434	8000.485225	10.382080	-0.051498	4.815773
250.783697	8000.414717	10.387085	-0.051522	4.815751
250.612253	8000.501604	10.392090	-0.051490	4.815778
250.733641	8000.382926	10.397095	-0.051513	4.815742
250.800111	8000.483282	10.402099	-0.051525	4.815771
250.739682	8000.514320	10.407104	-0.051514	4.815781
250.689620	8000.517769	10.412109	-0.051504	4.815782
250.924234	8000.429753	10.417114	-0.051548	4.815755
250.966239	8000.483805	10.422119	-0.051555	4.815771
250.866451	8000.472569	10.427123	-0.051537	4.815768
250.802931	8000.398932	10.432128	-0.051525	4.815747
250.869033	8000.514229	10.437133	-0.051537	4.815780
250.761936	8000.420668	10.442138	-0.051517	4.815753
250.844988	8000.439088	10.447143	-0.051532	4.815758
251.033714	8000.497657	10.452147	-0.051567	4.815774
250.951893	8000.413047	10.457152	-0.051552	4.815750
251.166096	8000.348187	10.462157	-0.051592	4.815730
251.157950	8000.479361	10.467162	-0.051590	4.815769
250.921945	8000.284422	10.472167	-0.051546	4.815713
250.733935	8000.471395	10.477171	-0.051511	4.815768
250.863501	8000.523665	10.482176	-0.051535	4.815783
250.888660	8000.457873	10.487181	-0.051540	4.815764
250.837783	8000.567001	10.492186	-0.051530	4.815796
250.816671	8000.420388	10.497191	-0.051526	4.815753
250.950686	8000.376646	10.502195	-0.051551	4.815739
250.698501	8000.508131	10.507200	-0.051504	4.815779
250.795769	8000.454184	10.512205	-0.051522	4.815763
250.785848	8000.418784	10.517210	-0.051520	4.815753
250.787198	8000.411323	10.522215	-0.051520	4.815750
250.705879	8000.377967	10.527219	-0.051505	4.815741
250.736298	8000.486278	10.532224	-0.051510	4.815773
250.958132	8000.367095	10.537229	-0.051551	4.815737
250.790173	8000.394253	10.542234	-0.051520	4.815745
250.848442	8000.494476	10.547239	-0.051531	4.815774
250.959917	8000.461045	10.552243	-0.051551	4.815764
251.059622	8000.429558	10.557248	-0.051570	4.815754
250.970890	8000.485759	10.562253	-0.051553	4.815771
251.028196	8000.374582	10.567258	-0.051564	4.815739
251.123575	8000.351565	10.572263	-0.051581	4.815731
251.007681	8000.480991	10.577267	-0.051560	4.815770
250.896587	8000.518680	10.582272	-0.051539	4.815781
250.934980	8000.377303	10.587277	-0.051546	4.815740
250.799569	8000.491465	10.592282	-0.051521	4.815774
250.953422	8000.408545	10.597287	-0.051549	4.815749
250.926447	8000.470019	10.602291	-0.051544	4.815767
250.982373	8000.431416	10.607296	-0.051554	4.815755
250.990861	8000.390975	10.612301	-0.051556	4.815744
251.058614	8000.506299	10.617306	-0.051568	4.815777
251.018921	8000.406359	10.622311	-0.051561	4.815748
250.930839	8000.381433	10.627315	-0.051544	4.815741
251.010905	8000.601582	10.632320	-0.051559	4.815805
251.268838	8000.415724	10.637325	-0.051607	4.815749
251.075132	8000.493710	10.642330	-0.051571	4.815773
251.123011	8000.411204	10.647335	-0.051580	4.815749
251.158527	8000.485436	10.652339	-0.051586	4.815770
250.975683	8000.363957	10.657344	-0.051552	4.815736
250.924270	8000.379127	10.662349	-0.051542	4.815740
250.941239	8000.535263	10.667354	-0.051546	4.815786
251.092481	8000.539844	10.672359	-0.051574	4.815787
251.223247	8000.376477	10.677363	-0.051598	4.815738
251.004646	8000.515980	10.682368	-0.051557	4.815780
251.085627	8000.384902	10.687373	-0.051572	4.815741
251.028836	8000.417067	10.692378	-0.051561	4.815751
251.175725	8000.452537	10.697383	-0.051589	4.815761
251.259446	8000.406912	10.702387	-0.051604	4.815747
251.046941	8000.391711	10.707392	-0.051564	4.815744
251.169942	8000.373413	10.712397	-0.051587	4.815738
251.072950	8000.401723	10.717402	-0.051569	4.815746
251.204996	8000.209553	10.722407	-0.051593	4.815690
251.222897	8000.368907	10.727411	-0.051597	4.815736
251.093073	8000.391346	10.732416	-0.051572	4.815743
251.300963	8000.393642	10.737421	-0.051611	4.815743
251.267311	8000.364262	10.742426	-0.051605	4.815734
251.255990	8000.384354	10.747431	-0.051602	4.815740
251.059334	8000.406776	10.752435	-0.051566	4.815748
250.872289	8000.497681	10.757440	-0.051531	4.815775
251.150252	8000.427450	10.762445	-0.051582	4.815754
251.166894	8000.385006	10.767450	-0.051585	4.815741
251.066519	8000.391909	10.772455	-0.051567	4.815744
251.255454	8000.390695	10.777459	-0.051602	4.815742
251.254811	8000.451529	10.782464	-0.051602	4.815760
251.048454	8000.423617	10.787469	-0.051563	4.815753
251.060311	8000.580738	10.792474	-0.051565	4.815799
251.088692	8000.410373	10.797479	-0.051570	4.815749
251.107692	8000.502486	10.802483	-0.051574	4.815776
251.348276	8000.385741	10.807488	-0.051618	4.815740
251.246624	8000.353122	10.812493	-0.051599	4.815731
251.025126	8000.339911	10.817498	-0.051558	4.815729
251.038887	8000.379626	10.822503	-0.051560	4.815740
251.142798	8000.358883	10.827507	-0.051580	4.815734
251.225065	8000.511809	10.832512	-0.051595	4.815778
251.244266	8000.419229	10.837517	-0.051598	4.815751
251.306933	8000.445860	10.842522	-0.051610	4.815758
251.212099	8000.336484	10.847527	-0.051592	4.815727
251.066086	8000.351187	10.852531	-0.051565	4.815732
251.171671	8000.510897	10.857536	-0.051584	4.815778
251.338327	8000.370532	10.862541	-0.051615	4.815736
251.153893	8000.381409	10.867546	-0.051581	4.815740
251.247352	8000.375443	10.872551	-0.051598	4.815738
251.353240	8000.388896	10.877555	-0.051618	4.815741
251.463633	8000.387475	10.882560	-0.051638	4.815740
251.394012	8000.245413	10.887565	-0.051625	4.815699
251.434396	8000.298371	10.892570	-0.051633	4.815715
251.430437	8000.355949	10.897575	-0.051632	4.815731
251.422608	8000.351542	10.902579	-0.051630	4.815730
251.280932	8000.504037	10.907584	-0.051604	4.815775
251.371430	8000.400871	10.912589	-0.051620	4.815745
251.144139	8000.500731	10.917594	-0.051578	4.815775
251.062296	8000.400107	10.922599	-0.051563	4.815746
251.266448	8000.340421	10.927603	-0.051601	4.815728
251.138184	8000.403455	10.932608	-0.051577	4.815747
251.166158	8000.379345	10.937613	-0.051582	4.815739
251.214915	8000.428169	10.942618	-0.051591	4.815754
251.272858	8000.329813	10.947623	-0.051601	4.815724
251.301199	8000.395387	10.952627	-0.051607	4.815744
251.253266	8000.396736	10.957632	-0.051598	4.815744
251.454461	8000.403194	10.962637	-0.051635	4.815745
251.491811	8000.492403	10.967642	-0.051642	4.815771
251.403942	8000.369260	10.972647	-0.051625	4.815735
251.233988	8000.375034	10.977651	-0.051593	4.815738
251.386300	8000.395646	10.982656	-0.051622	4.815743
251.486622	8000.247799	10.987661	-0.051640	4.815700
251.331411	8000.510039	10.992666	-0.051611	4.815777
251.283773	8000.359791	10.997671	-0.051602	4.815733
251.314954	8000.392316	11.002675	-0.051608	4.815743
251.409618	8000.371423	11.007680	-0.051626	4.815736
251.517063	8000.426538	11.012685	-0.051645	4.815752
251.288135	8000.335270	11.017690	-0.051603	4.815726
251.247096	8000.395449	11.022695	-0.051595	4.815744
251.334533	8000.343478	11.027699	-0.051611	4.815728
251.446098	8000.381578	11.032704	-0.051632	4.815739
251.354241	8000.402498	11.037709	-0.051615	4.815745
251.247586	8000.354851	11.042714	-0.051595	4.815732
251.435753	8000.333340	11.047719	-0.051630	4.815725
251.459874	8000.504540	11.052723	-0.051634	4.815775
251.264767	8000.383928	11.057728	-0.051598	4.815740
251.497784	8000.400511	11.062733	-0.051641	4.815744
251.452130	8000.484102	11.067738	-0.051632	4.815769
251.585553	8000.295156	11.072743	-0.051657	4.815713
251.476676	8000.365977	11.077747	-0.051637	4.815734
251.369111	8000.368493	11.082752	-0.051616	4.815735
251.373976	8000.255397	11.087757	-0.051617	4.815702
251.240115	8000.450723	11.092762	-0.051592	4.815760
251.568870	8000.404803	11.097767	-0.051653	4.815745
251.445014	8000.398514	11.102771	-0.051630	4.815744
251.329407	8000.281327	11.107776	-0.051608	4.815710
251.446383	8000.337664	11.112781	-0.051630	4.815726
251.294850	8000.372562	11.117786	-0.051602	4.815737
251.304257	8000.211498	11.122791	-0.051603	4.815690
251.263940	8000.170266	11.127795	-0.051596	4.815678
251.465319	8000.326191	11.132800	-0.051633	4.815723
251.450098	8000.270419	11.137805	-0.051630	4.815706
251.485846	8000.330776	11.142810	-0.051637	4.815724
251.443007	8000.366370	11.147815	-0.051629	4.815734
251.388128	8000.308888	11.152819	-0.051618	4.815718
251.222422	8000.470601	11.157824	-0.051588	4.815766
251.238544	8000.367296	11.162829	-0.051590	4.815736
251.431401	8000.472906	11.167834	-0.051626	4.815766
251.577388	8000.354626	11.172839	-0.051653	4.815730
251.482095	8000.279406	11.177843	-0.051635	4.815709
251.488846	8000.315805	11.182848	-0.051637	4.815720
251.485054	8000.280503	11.187853	-0.051636	4.815709
251.387520	8000.411295	11.192858	-0.051618	4.815748
251.458177	8000.385742	11.197863	-0.051631	4.815740
251.430105	8000.341505	11.202867	-0.051625	4.815727
251.225889	8000.405441	11.207872	-0.051587	4.815747
251.373762	8000.302139	11.212877	-0.051615	4.815716
251.514256	8000.443198	11.217882	-0.051641	4.815757
251.614342	8000.325241	11.222887	-0.051659	4.815722
251.444168	8000.379054	11.227891	-0.051627	4.815738
251.591850	8000.375035	11.232896	-0.051655	4.815736
251.701981	8000.306351	11.237901	-0.051675	4.815716
251.401024	8000.307864	11.242906	-0.051619	4.815718
251.365056	8000.341435	11.247911	-0.051612	4.815728
251.342344	8000.472373	11.252915	-0.051608	4.815766
251.420009	8000.352984	11.257920	-0.051622	4.815731
251.385549	8000.262737	11.262925	-0.051616	4.815705
251.351826	8000.395631	11.267930	-0.051609	4.815744
251.328391	8000.411256	11.272935	-0.051605	4.815748
251.467222	8000.271508	11.277939	-0.051631	4.815707
251.420959	8000.349751	11.282944	-0.051622	4.815730
251.674072	8000.193708	11.287949	-0.051669	4.815683
251.584936	8000.335312	11.292954	-0.051652	4.815725
251.548874	8000.268526	11.297959	-0.051645	4.815705
251.567675	8000.215441	11.302963	-0.051649	4.815690
251.480156	8000.336787	11.307968	-0.051632	4.815726
251.544990	8000.500107	11.312973	-0.051644	4.815773
251.385083	8000.352307	11.317978	-0.051614	4.815731
251.433360	8000.336000	11.322983	-0.051623	4.815726
251.472116	8000.315267	11.327987	-0.051630	4.815720
251.351652	8000.402983	11.332992	-0.051608	4.815746
251.515594	8000.207059	11.337997	-0.051638	4.815688
251.469466	8000.358969	11.343002	-0.051630	4.815732
251.486074	8000.266348	11.348007	-0.051633	4.815705
251.672809	8000.339830	11.353011	-0.051667	4.815726
251.359394	8000.397724	11.358016	-0.051609	4.815744
251.402135	8000.204105	11.363021	-0.051617	4.815687
251.478425	8000.514940	11.368026	-0.051631	4.815778
251.477810	8000.335562	11.373031	-0.051631	4.815725
251.563343	8000.386051	11.378035	-0.051646	4.815740
251.541247	8000.303477	11.383040	-0.051642	4.815716
251.696003	8000.254734	11.388045	-0.051671	4.815701
251.581052	8000.391649	11.393050	-0.051649	4.815741
251.377461	8000.374457	11.398055	-0.051611	4.815737
251.571460	8000.445923	11.403059	-0.051647	4.815757
251.629774	8000.376397	11.408064	-0.051658	4.815737
251.785251	8000.271083	11.413069	-0.051687	4.815705
251.600512	8000.414338	11.418074	-0.051652	4.815748
251.515402	8000.438571	11.423079	-0.051637	4.815755
251.564730	8000.301640	11.428083	-0.051646	4.815715
251.501589	8000.501317	11.433088	-0.051634	4.815774
251.768046	8000.252608	11.438093	-0.051683	4.815700
251.594935	8000.419540	11.443098	-0.051651	4.815749
251.640643	8000.261199	11.448103	-0.051659	4.815703
251.717325	8000.332896	11.453107	-0.051673	4.815724
251.576024	8000.393583	11.458112	-0.051647	4.815742
251.644052	8000.235604	11.463117	-0.051660	4.815695
251.730457	8000.351231	11.468122	-0.051676	4.815729
251.785956	8000.254970	11.473127	-0.051686	4.815700
251.814106	8000.203105	11.478131	-0.051691	4.815685
251.712605	8000.344508	11.483136	-0.051672	4.815727
251.739146	8000.280873	11.488141	-0.051677	4.815708
251.591550	8000.388433	11.493146	-0.051649	4.815740
251.670735	8000.403588	11.498151	-0.051664	4.815744
251.614370	8000.358892	11.503155	-0.051653	4.815732
251.613798	8000.533962	11.508160	-0.051653	4.815783
251.731466	8000.362909	11.513165	-0.051675	4.815732
251.739976	8000.375849	11.518170	-0.051676	4.815736
251.690430	8000.381441	11.523175	-0.051667	4.815738
251.652594	8000.394697	11.528179	-0.051660	4.815742
251.532280	8000.506970	11.533184	-0.051637	4.815775
251.679527	8000.230704	11.538189	-0.051665	4.815694
251.683357	8000.450685	11.543194	-0.051665	4.815758
251.830590	8000.305734	11.548199	-0.051693	4.815715
251.920127	8000.387249	11.553203	-0.051709	4.815739
251.780606	8000.395652	11.558208	-0.051683	4.815742
251.655722	8000.354115	11.563213	-0.051660	4.815730
251.730484	8000.398023	11.568218	-0.051674	4.815743
251.911882	8000.499179	11.573223	-0.051707	4.815771
251.832856	8000.282229	11.578227	-0.051692	4.815708
251.764495	8000.454064	11.583232	-0.051680	4.815759
251.754928	8000.384504	11.588237	-0.051678	4.815739
251.585600	8000.421249	11.593242	-0.051646	4.815750
251.657869	8000.428818	11.598247	-0.051659	4.815752
251.834170	8000.377222	11.603251	-0.051692	4.815736
251.740576	8000.467509	11.608256	-0.051675	4.815763
251.810124	8000.294607	11.613261	-0.051687	4.815712
251.723637	8000.375400	11.618266	-0.051671	4.815736
251.912554	8000.386998	11.623271	-0.051706	4.815739
251.879665	8000.393929	11.628275	-0.051700	4.815741
251.876952	8000.514517	11.633280	-0.051700	4.815776
251.888250	8000.404726	11.638285	-0.051701	4.815744
251.998033	8000.435324	11.643290	-0.051722	4.815752
251.788975	8000.483168	11.648295	-0.051683	4.815767
251.769077	8000.506323	11.653299	-0.051679	4.815774
252.009642	8000.387442	11.658304	-0.051724	4.815738
251.876599	8000.401288	11.663309	-0.051699	4.815743
251.946934	8000.400285	11.668314	-0.051712	4.815742
252.011830	8000.395991	11.673319	-0.051724	4.815741
252.035856	8000.392101	11.678323	-0.051728	4.815739
251.800455	8000.346635	11.683328	-0.051684	4.815727
251.867141	8000.437388	11.688333	-0.051696	4.815754
251.802779	8000.469430	11.693338	-0.051684	4.815763
251.777349	8000.418830	11.698343	-0.051680	4.815749
251.931610	8000.271858	11.703347	-0.051708	4.815705
251.995913	8000.392466	11.708352	-0.051720	4.815740
251.965819	8000.244637	11.713357	-0.051714	4.815697
252.018927	8000.232678	11.718362	-0.051724	4.815693
251.933953	8000.397838	11.723367	-0.051708	4.815742
251.895484	8000.262685	11.728371	-0.051701	4.815702
251.829764	8000.331004	11.733376	-0.051689	4.815723
252.011420	8000.388392	11.738381	-0.051722	4.815739
251.808391	8000.450212	11.743386	-0.051684	4.815758
251.618471	8000.456729	11.748391	-0.051649	4.815760
251.790378	8000.320720	11.753395	-0.051681	4.815720
251.862165	8000.413691	11.758400	-0.051694	4.815747
251.994369	8000.408354	11.763405	-0.051719	4.815744
252.076305	8000.303980	11.768410	-0.051734	4.815714
251.891718	8000.291367	11.773415	-0.051699	4.815711
252.026399	8000.214540	11.778419	-0.051724	4.815688
252.012945	8000.379793	11.783424	-0.051722	4.815736
252.151567	8000.172781	11.788429	-0.051747	4.815675
252.119065	8000.368686	11.793434	-0.051741	4.815732
251.875287	8000.261162	11.798439	-0.051696	4.815702
252.255202	8000.314293	11.803443	-0.051766	4.815716
252.067838	8000.383841	11.808448	-0.051731	4.815737
251.915244	8000.190253	11.813453	-0.051703	4.815681
251.867091	8000.299426	11.818458	-0.051694	4.815713
252.051019	8000.239412	11.823463	-0.051728	4.815695
252.139024	8000.174639	11.828467	-0.051744	4.815675
251.938881	8000.317645	11.833472	-0.051707	4.815718
251.937264	8000.252485	11.838477	-0.051706	4.815699
252.068945	8000.404080	11.843482	-0.051731	4.815743
252.034687	8000.368283	11.848487	-0.051724	4.815733
252.093801	8000.272080	11.853491	-0.051735	4.815704
252.133822	8000.353859	11.858496	-0.051743	4.815728
251.988018	8000.248993	11.863501	-0.051715	4.815698
251.925044	8000.310951	11.868506	-0.051703	4.815716
251.893753	8000.198335	11.873511	-0.051697	4.815684
251.862212	8000.194611	11.878515	-0.051691	4.815683
251.723291	8000.346083	11.883520	-0.051666	4.815728
252.001194	8000.382613	11.888525	-0.051717	4.815737
251.906047	8000.325543	11.893530	-0.051699	4.815721
251.875849	8000.304759	11.898535	-0.051694	4.815715
252.276192	8000.067831	11.903539	-0.051768	4.815644
252.220053	8000.265487	11.908544	-0.051757	4.815702
251.894092	8000.105386	11.913549	-0.051697	4.815656
251.750565	8000.405181	11.918554	-0.051670	4.815745
251.912704	8000.394991	11.923559	-0.051700	4.815741
252.024370	8000.396795	11.928563	-0.051721	4.815741
251.780032	8000.389617	11.933568	-0.051675	4.815740
251.916542	8000.261574	11.938573	-0.051700	4.815702
252.032074	8000.266643	11.943578	-0.051722	4.815703
251.802837	8000.271455	11.948583	-0.051679	4.815705
251.864874	8000.223342	11.953587	-0.051690	4.815691
251.952417	8000.283472	11.958592	-0.051707	4.815708
252.125772	8000.272397	11.963597	-0.051739	4.815704
252.116982	8000.385413	11.968602	-0.051737	4.815737
252.056073	8000.216799	11.973607	-0.051726	4.815688
251.799348	8000.335400	11.978611	-0.051678	4.815724
251.871535	8000.329089	11.983616	-0.051691	4.815722
252.175066	8000.296639	11.988621	-0.051747	4.815711
251.917660	8000.347968	11.993626	-0.051699	4.815727
251.901950	8000.484360	11.998631	-0.051696	4.815767
251.960753	8000.282457	12.003635	-0.051707	4.815708
251.924075	8000.488971	12.008640	-0.051700	4.815769
251.876724	8000.204208	12.013645	-0.051691	4.815685
252.038131	8000.358419	12.018650	-0.051721	4.815730
251.982847	8000.192032	12.023655	-0.051711	4.815681
252.210201	8000.112439	12.028659	-0.051753	4.815657
251.803028	8000.228598	12.033664	-0.051677	4.815693
251.797414	8000.205010	12.038669	-0.051676	4.815686
252.117746	8000.402370	12.043674	-0.051736	4.815742
252.136563	8000.367434	12.048679	-0.051739	4.815732
252.162565	8000.427634	12.053683	-0.051744	4.815749
251.991986	8000.320230	12.058688	-0.051712	4.815719
252.141123	8000.199865	12.063693	-0.051739	4.815683
252.060729	8000.298907	12.068698	-0.051724	4.815712
251.969130	8000.253639	12.073703	-0.051707	4.815700
251.906220	8000.349762	12.078707	-0.051695	4.815728
252.006295	8000.152801	12.083712	-0.051714	4.815670
252.008960	8000.361020	12.088717	-0.051714	4.815731
251.963322	8000.388028	12.093722	-0.051706	4.815739
252.079608	8000.184924	12.098727	-0.051727	4.815679
252.047499	8000.306101	12.103731	-0.051721	4.815715
251.991449	8000.373510	12.108736	-0.051711	4.815734
252.217643	8000.318453	12.113741	-0.051753	4.815717
251.935627	8000.380059	12.118746	-0.051700	4.815737
251.937390	8000.412107	12.123751	-0.051700	4.815746
252.110640	8000.386084	12.128755	-0.051733	4.815738
252.135471	8000.346976	12.133760	-0.051737	4.815726
251.924986	8000.308320	12.138765	-0.051698	4.815716
251.915758	8000.478980	12.143770	-0.051696	4.815766
251.871125	8000.390701	12.148775	-0.051688	4.815740
251.964693	8000.338830	12.153779	-0.051705	4.815724
251.827897	8000.407063	12.158784	-0.051679	4.815745
251.981103	8000.351889	12.163789	-0.051708	4.815728
251.961803	8000.420962	12.168794	-0.051704	4.815749
252.103729	8000.257775	12.173799	-0.051730	4.815700
252.121603	8000.312505	12.178803	-0.051733	4.815716
252.002546	8000.379958	12.183808	-0.051711	4.815736
251.973891	8000.457421	12.188813	-0.051706	4.815759
252.021263	8000.542523	12.193818	-0.051715	4.815784
252.206156	8000.506013	12.198823	-0.051749	4.815772
252.141812	8000.383250	12.203827	-0.051737	4.815737
252.172275	8000.508647	12.208832	-0.051742	4.815773
252.232564	8000.241643	12.213837	-0.051753	4.815695
252.275983	8000.288246	12.218842	-0.051761	4.815708
252.246127	8000.491669	12.223847	-0.051756	4.815768
252.164037	8000.304561	12.228851	-0.051740	4.815714
252.269704	8000.403420	12.233856	-0.051760	4.815742
252.317561	8000.387106	12.238861	-0.051769	4.815737
252.211624	8000.291426	12.243866	-0.051749	4.815710
252.203050	8000.290210	12.248871	-0.051747	4.815709
252.097174	8000.379231	12.253875	-0.051727	4.815736
251.941220	8000.359609	12.258880	-0.051698	4.815731
252.251585	8000.268551	12.263885	-0.051756	4.815703
252.147022	8000.244425	12.268890	-0.051736	4.815696
252.027887	8000.483764	12.273895	-0.051714	4.815767
251.995215	8000.339096	12.278899	-0.051708	4.815724
252.195786	8000.464051	12.283904	-0.051745	4.815760
252.130446	8000.259066	12.288909	-0.051733	4.815700
252.134706	8000.490800	12.293914	-0.051734	4.815768
252.324100	8000.283542	12.298919	-0.051769	4.815707
252.161579	8000.291572	12.303923	-0.051738	4.815710
252.199489	8000.310327	12.308928	-0.051745	4.815715
252.339698	8000.300850	12.313933	-0.051771	4.815712
252.264166	8000.373281	12.318938	-0.051757	4.815733
252.160598	8000.423904	12.323943	-0.051738	4.815749
252.214361	8000.322276	12.328947	-0.051748	4.815719
252.227168	8000.447387	12.333952	-0.051750	4.815755
252.137768	8000.237741	12.338957	-0.051733	4.815694
252.002682	8000.251554	12.343962	-0.051708	4.815699
252.201334	8000.423452	12.348967	-0.051745	4.815748
252.285652	8000.221963	12.353971	-0.051760	4.815689
252.036663	8000.383394	12.358976	-0.051714	4.815737
252.008621	8000.248410	12.363981	-0.051709	4.815698
252.197673	8000.423356	12.368986	-0.051744	4.815748
252.162079	8000.424904	12.373991	-0.051737	4.815749
252.146827	8000.295465	12.378995	-0.051734	4.815711
252.099176	8000.403580	12.384000	-0.051725	4.815743
252.209599	8000.401093	12.389005	-0.051745	4.815742
252.195812	8000.384845	12.394010	-0.051743	4.815737
252.229624	8000.399264	12.399015	-0.051749	4.815741
252.209606	8000.359428	12.404019	-0.051745	4.815729
252.087731	8000.378793	12.409024	-0.051722	4.815736
252.353877	8000.084171	12.414029	-0.051772	4.815648
252.172054	8000.374805	12.419034	-0.051738	4.815734
252.040501	8000.352376	12.424039	-0.051713	4.815728
252.262597	8000.285509	12.429043	-0.051754	4.815708
252.336330	8000.264276	12.434048	-0.051768	4.815701
252.306660	8000.302220	12.439053	-0.051762	4.815712
252.258457	8000.275805	12.444058	-0.051753	4.815705
252.102400	8000.487856	12.449063	-0.051724	4.815768
252.261343	8000.477615	12.454067	-0.051754	4.815764
252.102216	8000.466482	12.459072	-0.051724	4.815761
252.120287	8000.300217	12.464077	-0.051727	4.815713
252.319496	8000.387783	12.469082	-0.051764	4.815737
252.215948	8000.515276	12.474087	-0.051745	4.815775
252.239171	8000.254076	12.479091	-0.051749	4.815699
252.061520	8000.363284	12.484096	-0.051716	4.815731
252.345747	8000.247246	12.489101	-0.051769	4.815696
252.139400	8000.486238	12.494106	-0.051730	4.815767
251.942931	8000.500122	12.499111	-0.051694	4.815772
252.294700	8000.285892	12.504115	-0.051759	4.815708
252.018590	8000.381758	12.509120	-0.051707	4.815737
252.169019	8000.341486	12.514125	-0.051735	4.815724
252.110806	8000.435550	12.519130	-0.051724	4.815752
252.046299	8000.486807	12.524135	-0.051712	4.815768
252.275479	8000.304752	12.529139	-0.051755	4.815713
252.310063	8000.517762	12.534144	-0.051761	4.815775
252.420860	8000.401044	12.539149	-0.051782	4.815741
252.436563	8000.394884	12.544154	-0.051784	4.815739
252.386598	8000.407943	12.549159	-0.051775	4.815743
252.573767	8000.365064	12.554163	-0.051810	4.815729
252.430313	8000.486571	12.559168	-0.051783	4.815766
252.335158	8000.327008	12.564173	-0.051765	4.815720
252.178833	8000.286028	12.569178	-0.051736	4.815708
252.228352	8000.229171	12.574183	-0.051745	4.815691
252.309353	8000.219800	12.579187	-0.051760	4.815688
252.096950	8000.399974	12.584192	-0.051720	4.815742
252.327975	8000.311899	12.589197	-0.051763	4.815715
252.201362	8000.300227	12.594202	-0.051740	4.815712
251.995496	8000.379083	12.599207	-0.051701	4.815736
252.246502	8000.271048	12.604211	-0.051748	4.815704
252.337439	8000.349383	12.609216	-0.051765	4.815726
252.352419	8000.287695	12.614221	-0.051767	4.815708
252.352042	8000.362413	12.619226	-0.051767	4.815730
252.400386	8000.349310	12.624231	-0.051776	4.815726
252.439284	8000.385164	12.629235	-0.051783	4.815736
252.343988	8000.520264	12.634240	-0.051765	4.815776
252.500499	8000.411762	12.639245	-0.051794	4.815744
252.421192	8000.244984	12.644250	-0.051779	4.815695
252.052132	8000.489876	12.649255	-0.051711	4.815769
252.236156	8000.290005	12.654259	-0.051745	4.815709
252.143431	8000.364292	12.659264	-0.051727	4.815731
252.137008	8000.167738	12.664269	-0.051726	4.815674
252.362687	8000.312316	12.669274	-0.051768	4.815715
252.409471	8000.400612	12.674279	-0.051777	4.815741
252.545813	8000.193561	12.679283	-0.051802	4.815680
252.448564	8000.392687	12.684288	-0.051784	4.815738
252.523804	8000.225214	12.689293	-0.051798	4.815689
252.392382	8000.322361	12.694298	-0.051773	4.815718
252.291218	8000.502206	12.699303	-0.051754	4.815771
252.547253	8000.244784	12.704307	-0.051802	4.815695
252.565948	8000.476754	12.709312	-0.051805	4.815762
252.432156	8000.367810	12.714317	-0.051780	4.815731
252.395727	8000.383224	12.719322	-0.051773	4.815736
252.459198	8000.314849	12.724327	-0.051785	4.815715
252.372220	8000.169300	12.729331	-0.051768	4.815673
252.525641	8000.382102	12.734336	-0.051797	4.815735
252.640412	8000.349792	12.739341	-0.051818	4.815725
252.429501	8000.365577	12.744346	-0.051779	4.815730
252.320822	8000.491919	12.749351	-0.051759	4.815768
252.453332	8000.212207	12.754355	-0.051783	4.815685
252.423352	8000.361179	12.759360	-0.051777	4.815729
252.471375	8000.380099	12.764365	-0.051786	4.815734
252.170148	8000.383741	12.769370	-0.051730	4.815737
252.273472	8000.388612	12.774375	-0.051749	4.815738
252.537337	8000.214592	12.779379	-0.051798	4.815686
252.269801	8000.428036	12.784384	-0.051748	4.815749
252.496028	8000.243797	12.789389	-0.051790	4.815695
252.601763	8000.368281	12.794394	-0.051810	4.815730
252.533291	8000.384242	12.799399	-0.051797	4.815735
252.623887	8000.342999	12.804403	-0.051814	4.815723
252.490994	8000.381402	12.809408	-0.051789	4.815735
252.444740	8000.120143	12.814413	-0.051780	4.815659
252.391259	8000.337060	12.819418	-0.051770	4.815722
252.329808	8000.375556	12.824423	-0.051759	4.815734
252.399458	8000.256035	12.829427	-0.051771	4.815699
252.173095	8000.479756	12.834432	-0.051729	4.815765
252.333296	8000.432169	12.839437	-0.051759	4.815750
252.318371	8000.366792	12.844442	-0.051756	4.815731
252.375574	8000.420025	12.849447	-0.051767	4.815747
252.362583	8000.355748	12.854451	-0.051764	4.815728
252.422926	8000.387679	12.859456	-0.051775	4.815737
252.359761	8000.369563	12.864461	-0.051763	4.815732
252.510722	8000.401897	12.869466	-0.051791	4.815741
252.617503	8000.219990	12.874471	-0.051811	4.815687
252.719637	8000.213097	12.879475	-0.051830	4.815685
252.492560	8000.326841	12.884480	-0.051788	4.815719
252.603297	8000.376673	12.889485	-0.051808	4.815733
252.550975	8000.367273	12.894490	-0.051798	4.815730
252.510137	8000.377277	12.899495	-0.051791	4.815734
252.422500	8000.217838	12.904499	-0.051774	4.815687
252.419032	8000.464394	12.909504	-0.051774	4.815759
252.568838	8000.018415	12.914509	-0.051801	4.815628
252.380234	8000.367659	12.919514	-0.051766	4.815731
252.479438	8000.374598	12.924519	-0.051784	4.815733
252.645618	8000.295079	12.929523	-0.051815	4.815709
252.577852	8000.513902	12.934528	-0.051803	4.815773
252.687417	8000.225276	12.939533	-0.051823	4.815688
252.666979	8000.207853	12.944538	-0.051819	4.815683
252.541037	8000.348861	12.949543	-0.051795	4.815725
252.537559	8000.179044	12.954547	-0.051795	4.815675
252.499824	8000.238209	12.959552	-0.051787	4.815693
252.463986	8000.167155	12.964557	-0.051781	4.815672
252.472576	8000.329564	12.969562	-0.051782	4.815720
252.630374	8000.227489	12.974567	-0.051811	4.815689
252.706756	8000.152918	12.979571	-0.051825	4.815667
252.472755	8000.298578	12.984576	-0.051782	4.815711
252.664048	8000.349717	12.989581	-0.051817	4.815725
252.688138	8000.335152	12.994586	-0.051822	4.815720
252.523846	8000.392263	12.999591	-0.051791	4.815738
252.744056	8000.362732	13.004595	-0.051832	4.815728
252.591037	8000.387998	13.009600	-0.051803	4.815736
252.777082	8000.164671	13.014605	-0.051838	4.815670
252.635347	8000.394037	13.019610	-0.051812	4.815738
252.737929	8000.311350	13.024615	-0.051830	4.815713
252.745207	8000.212169	13.029619	-0.051832	4.815684
252.562425	8000.267913	13.034624	-0.051798	4.815701
252.665285	8000.322955	13.039629	-0.051817	4.815717
252.538668	8000.334769	13.044634	-0.051793	4.815721
252.456717	8000.399623	13.049639	-0.051778	4.815740
252.446900	8000.409063	13.054643	-0.051776	4.815743
252.564753	8000.432320	13.059648	-0.051798	4.815749
252.645371	8000.359953	13.064653	-0.051812	4.815728
252.730522	8000.369867	13.069658	-0.051828	4.815730
252.673629	8000.333702	13.074663	-0.051817	4.815720
252.746793	8000.340219	13.079667	-0.051831	4.815722
252.474406	8000.390237	13.084672	-0.051780	4.815738
252.595132	8000.378309	13.089677	-0.051803	4.815734
252.583122	8000.355684	13.094682	-0.051800	4.815727
252.696114	8000.472814	13.099687	-0.051821	4.815761
252.750107	8000.207841	13.104691	-0.051831	4.815683
252.490827	8000.442772	13.109696	-0.051783	4.815753
252.744561	8000.296346	13.114701	-0.051830	4.815709
252.658111	8000.269310	13.119706	-0.051814	4.815701
252.569622	8000.256121	13.124711	-0.051797	4.815698
252.728636	8000.218123	13.129715	-0.051826	4.815686
252.611983	8000.429746	13.134720	-0.051805	4.815749
252.530226	8000.356878	13.139725	-0.051789	4.815728
252.577196	8000.354429	13.144730	-0.051798	4.815727
252.647041	8000.470858	13.149735	-0.051811	4.815760
252.516809	8000.437773	13.154739	-0.051787	4.815751
252.551964	8000.345451	13.159744	-0.051793	4.815724
252.542358	8000.369841	13.164749	-0.051791	4.815731
252.681567	8000.264261	13.169754	-0.051817	4.815700
252.641644	8000.507024	13.174759	-0.051809	4.815771
252.763152	8000.391548	13.179763	-0.051832	4.815737
252.637040	8000.401235	13.184768	-0.051808	4.815740
252.602769	8000.129493	13.189773	-0.051802	4.815661
252.666009	8000.366455	13.194778	-0.051814	4.815730
252.792548	8000.430423	13.199783	-0.051837	4.815748
252.818363	8000.387060	13.204787	-0.051842	4.815735
252.499977	8000.382950	13.209792	-0.051782	4.815735
252.574006	8000.419374	13.214797	-0.051796	4.815746
252.607747	8000.341976	13.219802	-0.051802	4.815723
252.669189	8000.216984	13.224807	-0.051813	4.815686
252.627562	8000.325197	13.229811	-0.051806	4.815718
252.446217	8000.456765	13.234816	-0.051772	4.815757
252.322192	8000.214528	13.239821	-0.051748	4.815687
252.637842	8000.342418	13.244826	-0.051807	4.815723
252.656655	8000.405705	13.249831	-0.051811	4.815741
252.647418	8000.257145	13.254835	-0.051809	4.815698
252.588364	8000.486786	13.259840	-0.051798	4.815765
252.759825	8000.365714	13.264845	-0.051830	4.815729
252.531356	8000.525344	13.269850	-0.051787	4.815777
252.554645	8000.485143	13.274855	-0.051791	4.815765
252.709179	8000.342444	13.279859	-0.051820	4.815723
252.750634	8000.501119	13.284864	-0.051827	4.815769
252.619715	8000.140261	13.289869	-0.051803	4.815664
252.750124	8000.370840	13.294874	-0.051827	4.815731
252.809512	8000.368592	13.299879	-0.051838	4.815730
252.874367	8000.226573	13.304883	-0.051850	4.815688
252.864469	8000.401495	13.309888	-0.051848	4.815739
252.836965	8000.254774	13.314893	-0.051843	4.815696
252.792543	8000.301019	13.319898	-0.051834	4.815710
252.570215	8000.427652	13.324903	-0.051793	4.815748
252.641967	8000.238770	13.329907	-0.051806	4.815693
252.505631	8000.384948	13.334912	-0.051781	4.815736
252.538292	8000.518923	13.339917	-0.051787	4.815775
252.663448	8000.416317	13.344922	-0.051810	4.815744
252.651398	8000.390489	13.349927	-0.051808	4.815737
252.832735	8000.239685	13.354931	-0.051841	4.815692
252.838657	8000.498140	13.359936	-0.051842	4.815768
252.962231	8000.533234	13.364941	-0.051865	4.815777
252.851215	8000.428928	13.369946	-0.051844	4.815747
252.656734	8000.503699	13.374951	-0.051808	4.815770
252.712450	8000.360464	13.379955	-0.051818	4.815728
252.686129	8000.242588	13.384960	-0.051813	4.815694
252.528263	8000.312615	13.389965	-0.051784	4.815715
252.766269	8000.288711	13.394970	-0.051828	4.815707
252.905093	8000.337931	13.399975	-0.051854	4.815720
252.644359	8000.150058	13.404979	-0.051805	4.815667
252.564100	8000.337716	13.409984	-0.051790	4.815722
252.842863	8000.195966	13.414989	-0.051842	4.815679
252.623506	8000.341865	13.419994	-0.051801	4.815723
252.702295	8000.395448	13.424999	-0.051815	4.815738
252.879557	8000.256322	13.430003	-0.051848	4.815697
252.762563	8000.370785	13.435008	-0.051826	4.815731
252.522592	8000.343393	13.440013	-0.051782	4.815724
252.768684	8000.232074	13.445018	-0.051827	4.815690
252.800281	8000.303041	13.450023	-0.051833	4.815711
252.794727	8000.195112	13.455027	-0.051832	4.815679
252.508718	8000.364483	13.460032	-0.051779	4.815730
252.665239	8000.215412	13.465037	-0.051808	4.815686
252.753530	8000.271285	13.470042	-0.051824	4.815702
252.565571	8000.204168	13.475047	-0.051789	4.815683
252.698318	8000.245815	13.480051	-0.051813	4.815695
252.701166	8000.334465	13.485056	-0.051814	4.815720
252.686522	8000.323542	13.490061	-0.051811	4.815717
252.638914	8000.209592	13.495066	-0.051802	4.815684
252.670141	8000.229306	13.500071	-0.051808	4.815690
252.609262	8000.119412	13.505075	-0.051796	4.815658
252.599889	8000.346654	13.510080	-0.051795	4.815724
252.645755	8000.218207	13.515085	-0.051803	4.815687
252.703511	8000.225541	13.520090	-0.051814	4.815689
252.676630	8000.409795	13.525095	-0.051809	4.815743
252.669501	8000.385115	13.530099	-0.051807	4.815735
252.591752	8000.387046	13.535104	-0.051793	4.815736
252.855398	8000.515164	13.540109	-0.051842	4.815773
252.743745	8000.256042	13.545114	-0.051821	4.815697
252.763258	8000.351368	13.550119	-0.051824	4.815725
252.750507	8000.233713	13.555123	-0.051822	4.815691
252.635400	8000.557463	13.560128	-0.051800	4.815786
252.882064	8000.297752	13.565133	-0.051846	4.815709
252.901596	8000.387742	13.570138	-0.051850	4.815735
252.728498	8000.363570	13.575143	-0.051817	4.815729
252.645502	8000.225557	13.580147	-0.051802	4.815689
252.793798	8000.278133	13.585152	-0.051829	4.815704
252.907772	8000.129439	13.590157	-0.051850	4.815660
252.763597	8000.247731	13.595162	-0.051823	4.815695
252.705987	8000.401593	13.600167	-0.051812	4.815740
252.981899	8000.415672	13.605171	-0.051864	4.815743
252.781722	8000.508501	13.610176	-0.051826	4.815771
252.852236	8000.523516	13.615181	-0.051839	4.815775
252.894195	8000.276496	13.620186	-0.051847	4.815703
252.880901	8000.268797	13.625191	-0.051844	4.815700
252.863612	8000.407300	13.630195	-0.051841	4.815741
252.781612	8000.396351	13.635200	-0.051826	4.815738
252.811933	8000.338114	13.640205	-0.051831	4.815721
252.667379	8000.414763	13.645210	-0.051804	4.815744
252.625055	8000.303033	13.650215	-0.051796	4.815712
252.816606	8000.258090	13.655219	-0.051832	4.815698
252.702841	8000.407838	13.660224	-0.051811	4.815742
252.755803	8000.355307	13.665229	-0.051820	4.815726
252.803811	8000.371024	13.670234	-0.051829	4.815731
252.740620	8000.360380	13.675239	-0.051817	4.815728
252.588734	8000.256481	13.680243	-0.051789	4.815698
252.544042	8000.237597	13.685248	-0.051780	4.815693
252.799570	8000.342092	13.690253	-0.051828	4.815722
252.688738	8000.387260	13.695258	-0.051807	4.815736
252.769724	8000.374686	13.700263	-0.051822	4.815732
252.914621	8000.238237	13.705267	-0.051849	4.815691
252.945784	8000.268627	13.710272	-0.051855	4.815700
252.860468	8000.187161	13.715277	-0.051839	4.815677
252.640935	8000.293554	13.720282	-0.051798	4.815709
252.636314	8000.487779	13.725287	-0.051797	4.815766
252.777139	8000.115318	13.730291	-0.051823	4.815656
252.659269	8000.352544	13.735296	-0.051801	4.815726
252.683183	8000.395628	13.740301	-0.051805	4.815739
252.628996	8000.349899	13.745306	-0.051795	4.815725
252.678298	8000.295173	13.750311	-0.051804	4.815709
252.706714	8000.182457	13.755315	-0.051809	4.815676
252.727114	8000.338652	13.760320	-0.051813	4.815722
252.548093	8000.382713	13.765325	-0.051780	4.815735
252.807358	8000.287623	13.770330	-0.051828	4.815706
252.766926	8000.518634	13.775335	-0.051820	4.815774
252.684783	8000.286682	13.780339	-0.051805	4.815707
252.701171	8000.376620	13.785344	-0.051808	4.815733
252.799574	8000.342976	13.790349	-0.051826	4.815723
252.841428	8000.335106	13.795354	-0.051834	4.815720
252.789716	8000.375895	13.800359	-0.051824	4.815732
252.859388	8000.294809	13.805363	-0.051837	4.815708
252.797264	8000.361052	13.810368	-0.051825	4.815728
252.667495	8000.255377	13.815373	-0.051801	4.815698
252.879577	8000.250269	13.820378	-0.051840	4.815695
252.940291	8000.497869	13.825383	-0.051851	4.815767
253.079316	8000.197976	13.830387	-0.051877	4.815679
252.771320	8000.257025	13.835392	-0.051820	4.815698
252.878420	8000.245943	13.840397	-0.051839	4.815694
252.967545	8000.235636	13.845402	-0.051856	4.815690
252.795361	8000.339595	13.850407	-0.051824	4.815722
253.013640	8000.248110	13.855411	-0.051864	4.815694
252.952475	8000.384833	13.860416	-0.051853	4.815734
252.994397	8000.350272	13.865421	-0.051861	4.815724
253.132173	8000.242533	13.870426	-0.051886	4.815692
253.054911	8000.382198	13.875431	-0.051872	4.815733
253.016116	8000.026038	13.880435	-0.051864	4.815629
252.792397	8000.445179	13.885440	-0.051823	4.815753
253.040656	8000.291190	13.890445	-0.051869	4.815706
252.960767	8000.380633	13.895450	-0.051854	4.815733
252.589557	8000.356448	13.900455	-0.051784	4.815728
252.960668	8000.207656	13.905459	-0.051853	4.815682
252.845529	8000.255957	13.910464	-0.051832	4.815697
252.777732	8000.259118	13.915469	-0.051819	4.815698
252.774413	8000.350871	13.920474	-0.051818	4.815725
252.877879	8000.412329	13.925479	-0.051838	4.815743
252.990548	8000.426960	13.930483	-0.051859	4.815746
252.788234	8000.509078	13.935488	-0.051821	4.815771
252.898758	8000.500187	13.940493	-0.051841	4.815768
252.938224	8000.351349	13.945498	-0.051848	4.815724
252.920396	8000.434326	13.950503	-0.051845	4.815749
252.921013	8000.382012	13.955507	-0.051845	4.815734
252.872013	8000.381208	13.960512	-0.051836	4.815734
252.842037	8000.409538	13.965517	-0.051830	4.815742
252.974812	8000.255810	13.970522	-0.051855	4.815696
253.004786	8000.334224	13.975527	-0.051860	4.815719
253.071242	8000.213584	13.980531	-0.051872	4.815684
252.804388	8000.516722	13.985536	-0.051823	4.815774
252.888811	8000.262918	13.990541	-0.051838	4.815699
253.021296	8000.274668	13.995546	-0.051863	4.815702
252.892154	8000.521322	14.000551	-0.051839	4.815774
252.872254	8000.260487	14.005555	-0.051835	4.815698
252.982143	8000.320981	14.010560	-0.051855	4.815715
253.176275	8000.152234	14.015565	-0.051891	4.815665
253.002811	8000.120584	14.020570	-0.051859	4.815657
252.940871	8000.351245	14.025575	-0.051847	4.815724
253.030666	8000.217104	14.030579	-0.051864	4.815685
252.961379	8000.301381	14.035584	-0.051851	4.815710
253.127923	8000.163148	14.040589	-0.051882	4.815669
253.163225	8000.328127	14.045594	-0.051888	4.815717
252.963935	8000.369723	14.050599	-0.051851	4.815730
252.913775	8000.251460	14.055603	-0.051841	4.815695
252.858294	8000.365855	14.060608	-0.051831	4.815729
252.942082	8000.203858	14.065613	-0.051847	4.815681
253.020062	8000.308675	14.070618	-0.051861	4.815712
252.971036	8000.225662	14.075623	-0.051852	4.815688
253.113450	8000.200206	14.080627	-0.051878	4.815680
252.878895	8000.287139	14.085632	-0.051834	4.815706
252.927007	8000.265490	14.090637	-0.051843	4.815700
253.030608	8000.303462	14.095642	-0.051862	4.815710
253.014677	8000.398214	14.100647	-0.051859	4.815738
252.979397	8000.369873	14.105651	-0.051853	4.815730
253.021682	8000.328913	14.110656	-0.051860	4.815718
252.999323	8000.104339	14.115661	-0.051856	4.815652
252.926216	8000.209906	14.120666	-0.051842	4.815683
252.806747	8000.305111	14.125671	-0.051820	4.815712
252.961297	8000.307611	14.130675	-0.051849	4.815712
252.769738	8000.251111	14.135680	-0.051813	4.815696
252.826218	8000.189029	14.140685	-0.051823	4.815678
252.900261	8000.243603	14.145690	-0.051837	4.815693
252.728620	8000.297392	14.150695	-0.051805	4.815710
252.955106	8000.286112	14.155699	-0.051847	4.815705
252.910624	8000.259758	14.160704	-0.051839	4.815698
252.875108	8000.283727	14.165709	-0.051832	4.815705
252.826262	8000.358727	14.170714	-0.051823	4.815727
252.951663	8000.366092	14.175719	-0.051846	4.815729
252.996781	8000.279269	14.180723	-0.051854	4.815703
252.795096	8000.458551	14.185728	-0.051817	4.815757
252.992821	8000.258902	14.190733	-0.051853	4.815697
253.146330	8000.139674	14.195738	-0.051882	4.815662
252.794061	8000.205479	14.200743	-0.051816	4.815683
252.794068	8000.177712	14.205747	-0.051816	4.815675
252.829132	8000.403541	14.210752	-0.051823	4.815740
252.928993	8000.170274	14.215757	-0.051841	4.815672
252.876109	8000.298590	14.220762	-0.051831	4.815710
252.940842	8000.356216	14.225767	-0.051843	4.815726
252.852187	8000.300318	14.230771	-0.051826	4.815710
252.994784	8000.334653	14.235776	-0.051853	4.815720
252.923342	8000.331349	14.240781	-0.051839	4.815719
252.947142	8000.204678	14.245786	-0.051844	4.815682
252.804037	8000.241848	14.250791	-0.051817	4.815693
253.021755	8000.228291	14.255795	-0.051857	4.815688
252.846239	7999.465302	14.260800	-0.051824	4.815466

253.004171	7996.263293	14.265805	-0.051851	4.814529
253.017036	7990.698096	14.270810	-0.051850	4.812901
252.894592	7983.926306	14.275815	-0.051823	4.810919
252.936005	7976.664178	14.280819	-0.051826	4.808793
252.922639	7969.019723	14.285824	-0.051818	4.806554
252.696858	7961.232873	14.290829	-0.051771	4.804273
252.950059	7953.356975	14.295834	-0.051813	4.801963
252.814530	7945.368325	14.300839	-0.051782	4.799620
252.675321	7937.435695	14.305843	-0.051751	4.797293
252.579560	7929.387487	14.310848	-0.051728	4.794930
252.617151	7921.383450	14.315853	-0.051729	4.792578
252.444250	7913.361248	14.320858	-0.051692	4.790221
252.193463	7905.361089	14.325863	-0.051640	4.787870
252.530352	7897.377283	14.330867	-0.051697	4.785519
252.534438	7889.394893	14.335872	-0.051693	4.783170
252.358952	7881.415094	14.340877	-0.051655	4.780821
252.309392	7873.422941	14.345882	-0.051640	4.778466
252.283459	7865.402239	14.350887	-0.051630	4.776102
252.146107	7857.432785	14.355891	-0.051599	4.773752
252.105498	7849.338430	14.360896	-0.051586	4.771363
252.176699	7841.335172	14.365901	-0.051594	4.769000
252.083071	7833.396198	14.370906	-0.051571	4.766656
252.006703	7825.346258	14.375911	-0.051552	4.764277
251.989468	7817.415085	14.380915	-0.051543	4.761932
251.819249	7809.307742	14.385920	-0.051506	4.759534
251.665971	7801.405124	14.390925	-0.051473	4.757196
251.787253	7793.352483	14.395930	-0.051490	4.754811
251.783334	7785.351980	14.400935	-0.051484	4.752441
251.691903	7777.316623	14.405939	-0.051461	4.750059
251.621725	7769.324508	14.410944	-0.051443	4.747690
251.696321	7761.316891	14.415949	-0.051452	4.745313
251.710280	7753.343136	14.420954	-0.051449	4.742946
251.519145	7745.320859	14.425959	-0.051408	4.740564
251.687272	7737.327248	14.430963	-0.051434	4.738188
251.519025	7729.322788	14.435968	-0.051397	4.735809
251.403556	7721.284101	14.440973	-0.051370	4.733418
251.387080	7713.300789	14.445978	-0.051362	4.731042
251.360157	7705.285767	14.450983	-0.051352	4.728656
251.419570	7697.326916	14.455987	-0.051357	4.726285
251.278701	7689.269772	14.460992	-0.051326	4.723884
251.213039	7681.334653	14.465997	-0.051308	4.721517
251.216323	7673.312060	14.471002	-0.051304	4.719124
251.165087	7665.342244	14.476007	-0.051289	4.716745
251.252871	7657.376535	14.481011	-0.051300	4.714366
250.967555	7649.241680	14.486016	-0.051241	4.711935
250.921939	7641.252840	14.491021	-0.051227	4.709547
250.904438	7633.352806	14.496026	-0.051219	4.707184
251.071195	7625.256788	14.501031	-0.051245	4.704761
251.141938	7617.339339	14.506035	-0.051253	4.702390
250.843835	7609.317098	14.511040	-0.051192	4.699987
250.976772	7601.310247	14.516045	-0.051211	4.697587
250.937304	7593.324039	14.521050	-0.051198	4.695192
250.697205	7585.324045	14.526055	-0.051148	4.692792
250.672827	7577.262995	14.531059	-0.051139	4.690372
250.595570	7569.265049	14.536064	-0.051119	4.687970
250.456720	7561.244931	14.541069	-0.051088	4.685560
250.437512	7553.345916	14.546074	-0.051079	4.683185
250.305124	7545.283283	14.551079	-0.051049	4.680760
250.387476	7537.290264	14.556083	-0.051059	4.678354
250.307852	7529.347193	14.561088	-0.051039	4.675963
250.200805	7521.259956	14.566093	-0.051013	4.673526
250.066266	7513.115776	14.571098	-0.050983	4.671071
249.974113	7505.152045	14.576103	-0.050961	4.668670
250.091590	7497.228474	14.581107	-0.050977	4.666279
250.053257	7489.187371	14.586112	-0.050965	4.663851
249.922394	7481.243133	14.591117	-0.050935	4.661451
249.906348	7473.241479	14.596122	-0.050927	4.659033
250.030336	7465.276452	14.601127	-0.050944	4.656624
249.886119	7457.247622	14.606131	-0.050912	4.654196
249.921796	7449.214287	14.611136	-0.050914	4.651764
250.072474	7441.206070	14.616141	-0.050936	4.649338
249.799424	7433.256544	14.621146	-0.050880	4.646930
249.726681	7425.166557	14.626151	-0.050861	4.644477
249.660716	7417.280511	14.631155	-0.050844	4.642085
249.605213	7409.182617	14.636160	-0.050828	4.639627
249.524164	7401.264764	14.641165	-0.050808	4.637223
249.646612	7393.215763	14.646170	-0.050825	4.634778
249.645504	7385.183127	14.651175	-0.050820	4.632336
249.849185	7377.166259	14.656179	-0.050852	4.629898
249.639641	7369.223923	14.661184	-0.050808	4.627481
249.439993	7361.186393	14.666189	-0.050765	4.625034
249.666808	7353.206724	14.671194	-0.050802	4.622603
249.492103	7345.168555	14.676199	-0.050764	4.620153
249.499430	7337.248371	14.681203	-0.050761	4.617738
249.453483	7329.181956	14.686208	-0.050747	4.615277
249.315139	7321.144429	14.691213	-0.050715	4.612823
249.106184	7313.146013	14.696218	-0.050671	4.610380
249.104206	7305.167124	14.701223	-0.050666	4.607942
249.163414	7297.192419	14.706227	-0.050671	4.605504
248.997296	7289.178272	14.711232	-0.050635	4.603052
248.988393	7281.179501	14.716237	-0.050628	4.600604
249.308630	7273.237546	14.721242	-0.050682	4.598172
248.918771	7265.180588	14.726247	-0.050604	4.595703
248.749277	7257.180673	14.731251	-0.050568	4.593250
248.766467	7249.092146	14.736256	-0.050565	4.590769
248.701774	7241.127156	14.741261	-0.050548	4.588325
248.762559	7233.135658	14.746266	-0.050554	4.585871
248.785910	7225.143437	14.751271	-0.050553	4.583415
248.700930	7217.158841	14.756275	-0.050532	4.580961
248.724311	7209.142731	14.761280	-0.050531	4.578495
248.626496	7201.120159	14.766285	-0.050507	4.576026
248.561785	7193.167744	14.771290	-0.050490	4.573578
248.420507	7185.100338	14.776295	-0.050458	4.571092
248.467153	7177.144025	14.781299	-0.050462	4.568640
248.249907	7169.119120	14.786304	-0.050416	4.566165
248.360142	7161.138794	14.791309	-0.050431	4.563703
248.279077	7153.158504	14.796314	-0.050411	4.561239
248.198989	7145.153260	14.801319	-0.050391	4.558766
248.115891	7137.162512	14.806323	-0.050370	4.556296
247.958839	7129.133097	14.811328	-0.050335	4.553813
247.889433	7121.077427	14.816333	-0.050317	4.551320
248.010325	7113.098806	14.821338	-0.050334	4.548850
247.907366	7105.123681	14.826343	-0.050310	4.546380
247.794959	7097.130837	14.831347	-0.050283	4.543903
247.827102	7089.163707	14.836352	-0.050284	4.541432
247.800422	7081.116758	14.841357	-0.050274	4.538936
247.817520	7073.144364	14.846362	-0.050272	4.536461
247.838491	7065.105956	14.851367	-0.050270	4.533964
247.983355	7057.112336	14.856371	-0.050292	4.531480
247.609357	7049.104492	14.861376	-0.050217	4.528989
247.566898	7041.126982	14.866381	-0.050204	4.526507
247.533044	7033.138771	14.871386	-0.050192	4.524021
247.433722	7025.142429	14.876391	-0.050168	4.521530
247.448396	7017.136657	14.881395	-0.050166	4.519035
247.498368	7009.143043	14.886400	-0.050170	4.516543
247.370578	7001.099220	14.891405	-0.050141	4.514033
247.212657	6993.056175	14.896410	-0.050106	4.511522
247.276839	6985.029816	14.901415	-0.050112	4.509016
247.277254	6977.078362	14.906419	-0.050107	4.506531
247.116141	6969.033889	14.911424	-0.050072	4.504015
247.170265	6961.096815	14.916429	-0.050077	4.501532
247.166833	6953.106800	14.921434	-0.050071	4.499031
247.327258	6945.090812	14.926439	-0.050095	4.496521
247.141177	6937.076563	14.931443	-0.050055	4.494009
246.796287	6929.038555	14.936448	-0.049986	4.491488
246.903931	6921.042511	14.941453	-0.050001	4.488979
246.905625	6913.069869	14.946458	-0.049996	4.486477
246.843491	6905.032777	14.951463	-0.049979	4.483952
246.922828	6897.085169	14.956467	-0.049988	4.481455
246.674632	6889.048185	14.961472	-0.049937	4.478927
246.502291	6881.090418	14.966477	-0.049899	4.476423
246.447998	6873.073409	14.971482	-0.049884	4.473899
246.373993	6865.014602	14.976487	-0.049865	4.471361
246.577051	6857.048353	14.981491	-0.049897	4.468851
246.391767	6849.038567	14.986496	-0.049857	4.466325
246.444582	6841.003867	14.991501	-0.049862	4.463790
246.407283	6833.071695	14.996506	-0.049850	4.461286
246.130868	6825.043166	15.001511	-0.049793	4.458749
246.401947	6817.029317	15.006515	-0.049838	4.456217
246.386757	6809.030441	15.011520	-0.049830	4.453688
246.144057	6801.002538	15.016525	-0.049779	4.451147
246.274149	6793.022787	15.021530	-0.049798	4.448621
246.071458	6784.993780	15.026535	-0.049755	4.446077
246.108278	6777.052910	15.031539	-0.049757	4.443560
246.060472	6769.053709	15.036544	-0.049742	4.441023
246.010877	6761.026671	15.041549	-0.049728	4.438476
246.120014	6753.030562	15.046554	-0.049743	4.435938
245.750262	6745.007456	15.051559	-0.049669	4.433387
245.840143	6736.981544	15.056563	-0.049680	4.430837
245.674386	6728.976702	15.061568	-0.049644	4.428290
245.615870	6720.975939	15.066573	-0.049628	4.425744
245.630422	6713.019891	15.071578	-0.049625	4.423211
245.620699	6704.956109	15.076583	-0.049618	4.420642
245.683283	6697.004599	15.081587	-0.049624	4.418107
245.747378	6688.988136	15.086592	-0.049631	4.415551
245.742754	6681.001827	15.091597	-0.049625	4.413002
245.698652	6673.029566	15.096602	-0.049611	4.410456
245.541037	6664.973893	15.101607	-0.049576	4.407881
245.455763	6656.991134	15.106611	-0.049555	4.405328
245.577124	6648.997930	15.111616	-0.049573	4.402772
245.364011	6641.005154	15.116621	-0.049528	4.400213
245.260895	6633.052298	15.121626	-0.049503	4.397665
245.217232	6624.992053	15.126631	-0.049490	4.395082
245.266317	6617.005057	15.131635	-0.049493	4.392521
245.108692	6608.952379	15.136640	-0.049459	4.389937
245.144172	6600.974998	15.141645	-0.049460	4.387376
245.222248	6592.998594	15.146650	-0.049469	4.384815
245.014311	6584.986343	15.151655	-0.049425	4.382238
244.948418	6576.997657	15.156659	-0.049408	4.379669
245.176494	6568.986942	15.161664	-0.049445	4.377093
245.064865	6560.981365	15.166669	-0.049419	4.374515
245.142340	6553.019634	15.171674	-0.049428	4.371950
244.797867	6544.974709	15.176679	-0.049358	4.369355
244.779268	6537.029094	15.181683	-0.049350	4.366792
244.708978	6529.008892	15.186688	-0.049331	4.364203
244.659574	6521.047202	15.191693	-0.049317	4.361632
244.894078	6512.988993	15.196698	-0.049355	4.359030
244.425591	6505.053804	15.201703	-0.049262	4.356461
244.574208	6496.998170	15.206707	-0.049285	4.353856
244.356558	6488.871837	15.211712	-0.049239	4.351224
244.257741	6480.903220	15.216717	-0.049215	4.348643
244.293661	6472.987631	15.221722	-0.049217	4.346078
244.130037	6464.934587	15.226727	-0.049181	4.343465
244.372154	6456.969270	15.231731	-0.049221	4.340883
244.193529	6448.965665	15.236736	-0.049182	4.338283
244.229111	6440.996915	15.241741	-0.049183	4.335694
244.378193	6432.972844	15.246746	-0.049206	4.333087
244.208528	6424.931743	15.251751	-0.049169	4.330471
244.127818	6416.984720	15.256755	-0.049148	4.327884
243.850665	6408.950064	15.261760	-0.049092	4.325265
243.801448	6400.987108	15.266765	-0.049077	4.322670
243.943434	6392.999737	15.271770	-0.049098	4.320067
243.857363	6384.997472	15.276775	-0.049077	4.317456
243.836544	6376.997631	15.281779	-0.049068	4.314844
243.676823	6368.937081	15.286784	-0.049033	4.312210
243.683482	6360.923465	15.291789	-0.049028	4.309591
243.816070	6352.986189	15.296794	-0.049048	4.306997
243.534328	6344.908060	15.301799	-0.048990	4.304351
243.595478	6337.006933	15.306803	-0.048996	4.301764
243.550299	6328.953077	15.311808	-0.048982	4.299125
243.362722	6320.932423	15.316813	-0.048942	4.296495
243.345380	6312.942070	15.321818	-0.048934	4.293873
243.295113	6304.882310	15.326823	-0.048919	4.291227
243.505553	6296.933165	15.331827	-0.048953	4.288618
243.367373	6288.915888	15.336832	-0.048922	4.285982
243.182705	6280.924720	15.341837	-0.048882	4.283353
243.234308	6272.989408	15.346842	-0.048886	4.280742
243.146004	6264.936454	15.351847	-0.048865	4.278090
243.222351	6256.960050	15.356851	-0.048873	4.275463
242.939121	6248.909883	15.361856	-0.048815	4.272807
243.040176	6240.880264	15.366861	-0.048829	4.270159
243.101811	6232.922830	15.371866	-0.048835	4.267533
242.852916	6224.846281	15.376871	-0.048783	4.264864
243.045795	6216.929215	15.381875	-0.048814	4.262249
242.891817	6208.904592	15.386880	-0.048780	4.259594
242.688818	6200.948636	15.391885	-0.048737	4.256960
242.795186	6192.912827	15.396890	-0.048751	4.254300
242.597960	6184.931872	15.401895	-0.048709	4.251654
242.512397	6176.926496	15.406899	-0.048688	4.248999
242.599295	6168.922260	15.411904	-0.048699	4.246345
242.545659	6160.896889	15.416909	-0.048684	4.243681
242.468633	6153.012570	15.421914	-0.048664	4.241061
242.355972	6144.912553	15.426919	-0.048638	4.238368
242.442308	6136.986556	15.431923	-0.048648	4.235733
242.278060	6128.947064	15.436928	-0.048613	4.233057
242.079422	6120.950295	15.441933	-0.048570	4.230392
242.297562	6112.949188	15.446938	-0.048606	4.227728
242.407641	6104.908503	15.451943	-0.048621	4.225049
242.239572	6096.972866	15.456947	-0.048584	4.222400
242.099556	6088.956361	15.461952	-0.048553	4.219722
242.159217	6080.979151	15.466957	-0.048559	4.217058
242.102239	6072.965693	15.471962	-0.048543	4.214379
241.943219	6064.959552	15.476967	-0.048508	4.211700
241.886519	6056.919056	15.481971	-0.048492	4.209009
241.885955	6048.977987	15.486976	-0.048486	4.206349
241.753713	6040.933359	15.491981	-0.048456	4.203652
241.811208	6032.991317	15.496986	-0.048462	4.200990
241.635794	6024.983513	15.501991	-0.048424	4.198301
241.653654	6016.965482	15.506995	-0.048422	4.195609
241.529911	6008.910674	15.512000	-0.048393	4.192902
241.547140	6000.825957	15.517005	-0.048391	4.190184
241.504126	5992.909870	15.522010	-0.048378	4.187521
241.308893	5984.875846	15.527015	-0.048336	4.184814
241.580306	5976.930973	15.532019	-0.048382	4.182141
241.571135	5968.904015	15.537024	-0.048375	4.179436
241.382082	5960.938196	15.542029	-0.048334	4.176747
241.256083	5952.944048	15.547034	-0.048305	4.174048
241.246800	5944.918871	15.552039	-0.048298	4.171337
241.315663	5936.917530	15.557043	-0.048306	4.168634
241.114894	5928.915732	15.562048	-0.048263	4.165926
241.143430	5920.946459	15.567053	-0.048263	4.163230
241.199171	5912.906747	15.572058	-0.048268	4.160509
241.002753	5904.941775	15.577063	-0.048226	4.157808
240.990361	5896.951748	15.582067	-0.048219	4.155099
241.009155	5888.936419	15.587072	-0.048217	4.152380
240.895948	5880.895113	15.592077	-0.048190	4.149649
240.824594	5872.924750	15.597082	-0.048172	4.146941
240.704888	5864.891564	15.602087	-0.048144	4.144209
240.788698	5856.930800	15.607091	-0.048154	4.141502
240.900729	5848.916434	15.612096	-0.048170	4.138775
240.846951	5840.916951	15.617101	-0.048155	4.136050
240.672947	5832.925294	15.622106	-0.048117	4.133324
240.571500	5824.892420	15.627111	-0.048093	4.130583
240.630859	5816.919397	15.632115	-0.048098	4.127863
240.596066	5808.884707	15.637120	-0.048087	4.125119
240.328188	5800.947121	15.642125	-0.048031	4.122403
240.367421	5792.915842	15.647130	-0.048033	4.119657
240.361309	5784.965483	15.652135	-0.048027	4.116937
240.480646	5776.951871	15.657139	-0.048044	4.114195
240.249535	5768.913988	15.662144	-0.047995	4.111437
240.173444	5760.852047	15.667149	-0.047976	4.108672
240.378581	5752.898546	15.672154	-0.048009	4.105946
240.238237	5744.900778	15.677159	-0.047977	4.103199
240.115688	5736.968611	15.682163	-0.047949	4.100472
240.090743	5728.949938	15.687168	-0.047939	4.097715
240.016518	5720.924084	15.692173	-0.047920	4.094953
239.939203	5712.979957	15.697178	-0.047901	4.092217
239.805710	5704.911119	15.702183	-0.047870	4.089435
239.800279	5696.945983	15.707187	-0.047864	4.086690
239.619635	5688.965121	15.712192	-0.047825	4.083934
239.716781	5680.989493	15.717197	-0.047838	4.081182
239.669268	5672.988870	15.722202	-0.047824	4.078418
239.404844	5664.969934	15.727207	-0.047769	4.075643
239.523321	5656.962730	15.732211	-0.047786	4.072875
239.598112	5648.951886	15.737216	-0.047794	4.070103
239.297016	5640.953728	15.742221	-0.047733	4.067329
239.446155	5632.943572	15.747226	-0.047755	4.064554
239.421655	5624.954993	15.752231	-0.047746	4.061783
239.471732	5616.961599	15.757235	-0.047750	4.059010
239.372788	5608.961888	15.762240	-0.047726	4.056230
239.196631	5600.971839	15.767245	-0.047688	4.053450
239.348529	5592.974460	15.772250	-0.047711	4.050671
239.068130	5584.961311	15.777255	-0.047653	4.047878
238.998275	5576.959224	15.782259	-0.047635	4.045090
238.965196	5568.988883	15.787264	-0.047623	4.042312
238.847338	5560.951608	15.792269	-0.047596	4.039507
239.034934	5553.009677	15.797274	-0.047626	4.036738
238.830997	5544.962245	15.802279	-0.047582	4.033925
238.893968	5536.840179	15.807283	-0.047589	4.031087
238.959435	5528.895933	15.812288	-0.047596	4.028310
238.852659	5520.896021	15.817293	-0.047570	4.025508
238.976490	5512.968228	15.822298	-0.047588	4.022734
238.792181	5504.919655	15.827303	-0.047549	4.019910
238.587008	5496.978306	15.832307	-0.047505	4.017122
238.662483	5488.936687	15.837312	-0.047514	4.014301
238.636291	5480.915021	15.842317	-0.047504	4.011483
238.427351	5472.949847	15.847322	-0.047459	4.008681
238.274370	5464.924806	15.852327	-0.047426	4.005856
238.475696	5456.974570	15.857331	-0.047458	4.003061
238.328369	5448.965925	15.862336	-0.047425	4.000238
238.100597	5440.999443	15.867341	-0.047377	3.997427
238.328650	5432.980580	15.872346	-0.047414	3.994602
237.842820	5424.948036	15.877351	-0.047319	3.991760
238.062254	5416.951517	15.882355	-0.047354	3.988939
238.182781	5408.942208	15.887360	-0.047371	3.986110
238.009397	5400.938144	15.892365	-0.047334	3.983276
237.930498	5392.990095	15.897370	-0.047314	3.980462
237.752111	5384.978376	15.902375	-0.047275	3.977621
237.932734	5376.992478	15.907379	-0.047304	3.974793
237.721105	5368.979774	15.912384	-0.047259	3.971948
237.668121	5360.932820	15.917389	-0.047244	3.969090
237.577558	5353.001554	15.922394	-0.047221	3.966272
237.501955	5344.972532	15.927399	-0.047202	3.963416
237.512714	5337.007460	15.932403	-0.047199	3.960583
237.467069	5329.042055	15.937408	-0.047185	3.957747
237.437894	5321.034278	15.942413	-0.047174	3.954893
237.481960	5312.984078	15.947418	-0.047177	3.952024
237.464068	5304.948872	15.952423	-0.047168	3.949157
237.416216	5297.007531	15.957427	-0.047154	3.946321
237.358050	5289.004301	15.962432	-0.047138	3.943461
237.226218	5281.014926	15.967437	-0.047108	3.940602
237.319363	5273.059466	15.972442	-0.047120	3.937757
237.289947	5265.015609	15.977447	-0.047109	3.934877
237.236981	5256.993651	15.982451	-0.047094	3.932001
237.087111	5249.000748	15.987456	-0.047061	3.929133
237.278592	5241.011283	15.992461	-0.047091	3.926269
237.270361	5233.037707	15.997466	-0.047084	3.923406
237.133602	5225.026139	16.002471	-0.047054	3.920524
237.139572	5217.067033	16.007475	-0.047050	3.917662
236.979886	5209.041604	16.012480	-0.047014	3.914770
237.038789	5200.989256	16.017485	-0.047020	3.911871
237.096156	5193.053770	16.022490	-0.047025	3.909012
237.033194	5184.991016	16.027495	-0.047008	3.906103
236.703015	5177.031223	16.032499	-0.046942	3.903223
236.633793	5169.020610	16.037504	-0.046923	3.900328
236.716616	5161.042533	16.042509	-0.046934	3.897446
236.623763	5153.024374	16.047514	-0.046911	3.894543
236.460443	5145.011654	16.052519	-0.046875	3.891639
236.777382	5136.994153	16.057523	-0.046929	3.888740
236.451080	5129.027086	16.062528	-0.046863	3.885845
236.464994	5121.021256	16.067533	-0.046860	3.882941
236.445000	5113.055036	16.072538	-0.046851	3.880047
236.332190	5105.080017	16.077543	-0.046825	3.877147
236.514686	5097.030706	16.082547	-0.046853	3.874223
236.193715	5088.775464	16.087552	-0.046788	3.871212
236.186837	5080.864418	16.092557	-0.046782	3.868331
236.215693	5072.938489	16.097562	-0.046782	3.865442
236.076621	5064.981483	16.102567	-0.046750	3.862537
236.199359	5056.984500	16.107571	-0.046768	3.859620
235.945627	5049.062132	16.112576	-0.046715	3.856721
235.914523	5040.984129	16.117581	-0.046704	3.853767
235.988024	5033.019966	16.122586	-0.046713	3.850854
235.891794	5025.015871	16.127591	-0.046689	3.847921
235.936667	5017.034728	16.132595	-0.046693	3.844998
235.797668	5009.079330	16.137600	-0.046661	3.842077
235.789331	5001.053806	16.142605	-0.046654	3.839132
235.878691	4993.094354	16.147610	-0.046666	3.836210
235.773539	4985.064519	16.152615	-0.046641	3.833256
235.618824	4977.041202	16.157619	-0.046607	3.830302
235.746044	4969.065689	16.162624	-0.046625	3.827368
235.544672	4961.049006	16.167629	-0.046582	3.824411
235.591487	4953.141996	16.172634	-0.046586	3.821496
235.539446	4945.132531	16.177639	-0.046571	3.818540
235.523822	4937.122964	16.182643	-0.046563	3.815582
235.361231	4929.126470	16.187648	-0.046527	3.812623
235.376125	4921.080352	16.192653	-0.046524	3.809647
235.276458	4913.152611	16.197658	-0.046501	3.806711
235.060637	4905.117378	16.202663	-0.046455	3.803729
235.138056	4897.171459	16.207667	-0.046464	3.800785
235.082543	4889.143628	16.212672	-0.046448	3.797806
235.070788	4881.151474	16.217677	-0.046441	3.794838
234.997224	4873.101233	16.222682	-0.046422	3.791845
234.859720	4865.108193	16.227687	-0.046391	3.788869
234.907909	4857.077686	16.232691	-0.046395	3.785882
234.781292	4849.155322	16.237696	-0.046366	3.782928
234.927597	4841.116450	16.242701	-0.046388	3.779934
234.908442	4833.172518	16.247706	-0.046379	3.776970
234.505910	4825.151081	16.252711	-0.046299	3.773966
234.646712	4817.127398	16.257715	-0.046319	3.770972
234.806855	4809.124713	16.262720	-0.046344	3.767983
234.516221	4801.124208	16.267725	-0.046284	3.764982
234.488713	4793.179054	16.272730	-0.046274	3.762005
234.492115	4785.145060	16.277735	-0.046269	3.758994
234.453592	4777.195799	16.282739	-0.046257	3.756011
234.374739	4769.152305	16.287744	-0.046237	3.752989
234.371992	4761.108940	16.292749	-0.046231	3.749966
234.240816	4753.171359	16.297754	-0.046201	3.746978
234.175891	4745.145649	16.302759	-0.046184	3.743956
234.214817	4737.194505	16.307763	-0.046186	3.740962
234.262276	4729.200336	16.312768	-0.046189	3.737950
234.186431	4721.165785	16.317773	-0.046170	3.734917
234.105934	4713.172809	16.322778	-0.046150	3.731897
234.073122	4705.156063	16.327783	-0.046138	3.728867
233.917187	4697.181754	16.332787	-0.046104	3.725847
233.930069	4689.208969	16.337792	-0.046101	3.722830
233.735340	4681.225473	16.342797	-0.046059	3.719801
233.865490	4673.266376	16.347802	-0.046078	3.716786
233.652954	4665.213230	16.352807	-0.046033	3.713726
233.635177	4657.152585	16.357811	-0.046025	3.710664
233.544561	4649.191191	16.362816	-0.046003	3.707636
233.509871	4641.157228	16.367821	-0.045991	3.704579
233.395938	4633.271169	16.372826	-0.045964	3.701574
233.247291	4625.250500	16.377831	-0.045931	3.698515
233.242600	4617.253280	16.382835	-0.045925	3.695465
233.359702	4609.242387	16.387840	-0.045942	3.692411
233.135740	4601.205035	16.392845	-0.045895	3.689336
233.255057	4593.249725	16.397850	-0.045911	3.686297
233.270502	4585.248278	16.402855	-0.045909	3.683237
233.184544	4577.265941	16.407859	-0.045888	3.680178
233.202180	4569.297209	16.412864	-0.045886	3.677125
233.113810	4561.270593	16.417869	-0.045864	3.674044
232.999407	4553.286648	16.422874	-0.045837	3.670976
232.852772	4545.237688	16.427879	-0.045805	3.667880
233.046335	4537.252145	16.432883	-0.045835	3.664815
233.005498	4529.305307	16.437888	-0.045822	3.661755
233.014787	4521.296098	16.442893	-0.045819	3.658671
233.017899	4513.307829	16.447898	-0.045814	3.655592
232.818645	4505.262473	16.452903	-0.045772	3.652482
232.557830	4497.297786	16.457907	-0.045718	3.649400
232.559502	4489.331599	16.462912	-0.045713	3.646322
232.406807	4481.322274	16.467917	-0.045679	3.643219
232.468826	4473.352567	16.472922	-0.045685	3.640136
232.414053	4465.345332	16.477927	-0.045670	3.637032
232.518110	4457.318634	16.482931	-0.045684	3.633922
232.440094	4449.290551	16.487936	-0.045664	3.630804
231.955447	4441.309071	16.492941	-0.045568	3.627691
232.269092	4433.297181	16.497946	-0.045622	3.624584
232.184196	4425.340886	16.502951	-0.045600	3.621486
232.278224	4417.365212	16.507955	-0.045613	3.618382
232.176788	4409.374130	16.512960	-0.045588	3.615265
231.795484	4401.335431	16.517965	-0.045512	3.612118
231.820326	4393.366168	16.522970	-0.045511	3.609007
231.819950	4385.348874	16.527975	-0.045506	3.605874
231.619965	4377.415043	16.532979	-0.045464	3.602765
231.499146	4369.422701	16.537984	-0.045436	3.599633
231.388395	4361.458156	16.542989	-0.045410	3.596509
231.527910	4353.428454	16.547994	-0.045430	3.593364
231.471339	4345.396033	16.552999	-0.045415	3.590209
231.395675	4337.414186	16.558003	-0.045395	3.587071
231.609083	4329.395362	16.563008	-0.045430	3.583924
231.441219	4321.446133	16.568013	-0.045393	3.580791
231.393175	4313.499952	16.573018	-0.045379	3.577660
231.310778	4305.435829	16.578023	-0.045358	3.574478
231.362007	4297.427649	16.583027	-0.045362	3.571319
231.310294	4289.459392	16.588032	-0.045347	3.568171
231.002429	4281.449199	16.593037	-0.045285	3.564996
231.285717	4273.487756	16.598042	-0.045332	3.561854
231.266176	4265.474500	16.603047	-0.045323	3.558680
230.961761	4257.511628	16.608051	-0.045261	3.555515
230.891935	4249.418941	16.613056	-0.045243	3.552302
230.811291	4241.385504	16.618061	-0.045222	3.549110
230.773292	4233.436233	16.623066	-0.045210	3.545950
230.655407	4225.451434	16.628071	-0.045183	3.542770
230.742732	4217.474869	16.633075	-0.045194	3.539597
230.821711	4209.487259	16.638080	-0.045203	3.536416
230.617440	4201.468001	16.643085	-0.045160	3.533211
230.759600	4193.475947	16.648090	-0.045181	3.530025
230.559568	4185.488188	16.653095	-0.045138	3.526827
230.518684	4177.509676	16.658099	-0.045126	3.523635
230.389149	4169.560009	16.663104	-0.045096	3.520449
230.311886	4161.563751	16.668109	-0.045076	3.517242
230.312328	4153.567298	16.673114	-0.045071	3.514035
230.181796	4145.543152	16.678119	-0.045042	3.510810
230.367170	4137.532335	16.683123	-0.045071	3.507597
230.288566	4129.507316	16.688128	-0.045051	3.504368
230.229707	4121.589763	16.693133	-0.045035	3.501179
230.184212	4113.626520	16.698138	-0.045021	3.497969
230.155919	4105.591114	16.703143	-0.045010	3.494728
230.198682	4097.583910	16.708147	-0.045013	3.491497
230.127401	4089.607719	16.713152	-0.044994	3.488273
229.895866	4081.593660	16.718157	-0.044946	3.485024
229.946591	4073.662089	16.723162	-0.044950	3.481816
229.842936	4065.653722	16.728167	-0.044925	3.478568
229.927906	4057.661041	16.733171	-0.044936	3.475329
229.692651	4049.631997	16.738176	-0.044887	3.472063
229.525297	4041.596773	16.743181	-0.044850	3.468793
229.703336	4033.623003	16.748186	-0.044878	3.465556
229.658550	4025.636853	16.753191	-0.044864	3.462304
229.566620	4017.646694	16.758195	-0.044842	3.459045
229.332848	4009.725241	16.763200	-0.044793	3.455807
229.461403	4001.660602	16.768205	-0.044812	3.452519
229.519609	3993.694807	16.773210	-0.044817	3.449267
229.170022	3985.696249	16.778215	-0.044747	3.445984
229.177507	3977.716160	16.783219	-0.044743	3.442717
229.303212	3969.702051	16.788224	-0.044761	3.439438
229.176884	3961.734330	16.793229	-0.044732	3.436165
229.130481	3953.723648	16.798234	-0.044718	3.432875
229.058630	3945.722757	16.803239	-0.044700	3.429585
229.054684	3937.730079	16.808243	-0.044694	3.426297
228.895173	3929.766971	16.813248	-0.044659	3.423013
228.915951	3921.753560	16.818253	-0.044657	3.419711
228.988832	3913.809389	16.823258	-0.044665	3.416437
228.713258	3905.787558	16.828263	-0.044609	3.413115
228.892779	3897.772121	16.833267	-0.044637	3.409808
228.775541	3889.804918	16.838272	-0.044610	3.406508
228.499224	3881.808282	16.843277	-0.044553	3.403186
228.550034	3873.844927	16.848282	-0.044557	3.399887
228.536301	3865.856340	16.853287	-0.044549	3.396572
228.514895	3857.807088	16.858291	-0.044540	3.393228
228.392950	3849.747231	16.863296	-0.044512	3.389873
228.446133	3841.764616	16.868301	-0.044516	3.386552
228.470669	3833.830436	16.873306	-0.044516	3.383248
228.258198	3825.833542	16.878311	-0.044471	3.379906
228.167584	3817.879165	16.883315	-0.044449	3.376583
228.155061	3809.874484	16.888320	-0.044441	3.373238
228.061995	3801.842099	16.893325	-0.044418	3.369875
228.170680	3793.878040	16.898330	-0.044433	3.366545
228.123739	3785.886012	16.903335	-0.044419	3.363194
228.282013	3777.908147	16.908339	-0.044443	3.359853
228.019280	3769.967717	16.913344	-0.044389	3.356509
227.875311	3761.912974	16.918349	-0.044357	3.353119
227.923341	3753.905465	16.923354	-0.044361	3.349751
227.842063	3745.926093	16.928359	-0.044340	3.346388
227.785369	3737.936367	16.933363	-0.044324	3.343017
227.818689	3729.947631	16.938368	-0.044325	3.339647
227.635592	3721.986575	16.943373	-0.044286	3.336277
227.443753	3713.985718	16.948378	-0.044245	3.332886
227.693198	3705.933033	16.953383	-0.044286	3.329487
227.679333	3697.989653	16.958387	-0.044278	3.326120
227.446046	3690.011851	16.963392	-0.044229	3.322728
227.176512	3682.023466	16.968397	-0.044174	3.319326
227.340060	3674.088059	16.973402	-0.044199	3.315959
227.144076	3666.021625	16.978407	-0.044157	3.312519
227.029897	3658.018674	16.983411	-0.044131	3.309106
227.345639	3650.036265	16.988416	-0.044184	3.305715
227.341169	3642.058299	16.993421	-0.044178	3.302310
227.171395	3634.093124	16.998426	-0.044141	3.298900
227.092355	3626.088011	17.003431	-0.044121	3.295474
227.262146	3618.090788	17.008435	-0.044147	3.292056
227.091444	3610.098940	17.013440	-0.044110	3.288625
226.738126	3602.103624	17.018445	-0.044039	3.285181
227.021441	3594.156690	17.023450	-0.044087	3.281779
226.850247	3586.163221	17.028455	-0.044049	3.278335
226.811384	3578.183628	17.033459	-0.044037	3.274900
226.905714	3570.174244	17.038464	-0.044049	3.271453
226.768989	3562.153080	17.043469	-0.044018	3.267988
226.546418	3554.212658	17.048474	-0.043971	3.264551
226.494770	3546.218136	17.053479	-0.043957	3.261094
226.562636	3538.209620	17.058483	-0.043964	3.257631
226.285824	3530.234788	17.063488	-0.043907	3.254166
226.231896	3522.210635	17.068493	-0.043892	3.250685
226.536451	3514.220968	17.073498	-0.043943	3.247229
226.398456	3506.233201	17.078503	-0.043912	3.243753
226.168346	3498.283410	17.083507	-0.043864	3.240285
226.074591	3490.305931	17.088512	-0.043841	3.236808
226.086015	3482.255705	17.093517	-0.043838	3.233299
225.967465	3474.251365	17.098522	-0.043811	3.229801
225.765639	3466.267113	17.103527	-0.043768	3.226305
225.871523	3458.294904	17.108531	-0.043782	3.222822
225.935302	3450.278912	17.113536	-0.043789	3.219315
225.687254	3442.334414	17.118541	-0.043737	3.215823
225.803461	3434.339454	17.123546	-0.043753	3.212320
225.850800	3426.304968	17.128551	-0.043757	3.208793
225.878718	3418.340030	17.133555	-0.043757	3.205291
225.733495	3410.411542	17.138560	-0.043725	3.201795
225.579250	3402.403434	17.143565	-0.043690	3.198259
225.631649	3394.442583	17.148570	-0.043695	3.194749
225.552449	3386.408347	17.153575	-0.043675	3.191197
225.631116	3378.405408	17.158579	-0.043684	3.187662
225.555292	3370.416947	17.163584	-0.043665	3.184123
225.336183	3362.468059	17.168589	-0.043619	3.180591
225.426716	3354.499038	17.173594	-0.043630	3.177059
225.360354	3346.468246	17.178599	-0.043613	3.173489
225.220781	3338.490086	17.183603	-0.043581	3.169936
225.211016	3330.505581	17.188608	-0.043574	3.166381
225.253684	3322.495562	17.193613	-0.043577	3.162813
225.162755	3314.567686	17.198618	-0.043555	3.159273
224.765037	3306.600363	17.203623	-0.043475	3.155697
224.989564	3298.555774	17.208627	-0.043512	3.152109
224.941537	3290.541291	17.213632	-0.043497	3.148519
224.846925	3282.561422	17.218637	-0.043474	3.144938
224.824975	3274.611379	17.223642	-0.043465	3.141370
224.651182	3266.615848	17.228647	-0.043427	3.137771
224.663600	3258.625812	17.233651	-0.043424	3.134178
224.544358	3250.643373	17.238656	-0.043397	3.130579
224.462638	3242.629089	17.243661	-0.043376	3.126963
224.630268	3234.669250	17.248666	-0.043402	3.123378
224.414340	3226.683334	17.253671	-0.043357	3.119760
224.420662	3218.743324	17.258675	-0.043353	3.116169
224.397049	3210.710720	17.263680	-0.043343	3.112530
224.132264	3202.705409	17.268685	-0.043288	3.108889
224.314148	3194.718549	17.273690	-0.043317	3.105272
224.249484	3186.741586	17.278695	-0.043299	3.101643
224.104664	3178.776555	17.283699	-0.043267	3.098013
223.934324	3170.800900	17.288704	-0.043230	3.094372
223.925693	3162.773265	17.293709	-0.043223	3.090711
224.052155	3154.808476	17.298714	-0.043242	3.087080
223.826313	3146.818342	17.303719	-0.043194	3.083417
223.682125	3138.863628	17.308723	-0.043162	3.079769
223.762638	3130.890824	17.313728	-0.043172	3.076120
223.809318	3122.812548	17.318733	-0.043175	3.072416
223.546053	3114.829258	17.323738	-0.043121	3.068736
223.528978	3106.829850	17.328743	-0.043112	3.065057
223.540363	3098.873064	17.333747	-0.043109	3.061394
223.353890	3090.922395	17.338752	-0.043069	3.057720
223.252088	3082.915896	17.343757	-0.043045	3.054019
223.239348	3074.928218	17.348762	-0.043037	3.050328
223.024197	3066.963674	17.353767	-0.042992	3.046633
223.303446	3058.954459	17.358771	-0.043038	3.042936
223.187244	3050.982986	17.363776	-0.043011	3.039233
222.981011	3043.052798	17.368781	-0.042968	3.035541
223.184573	3035.021342	17.373786	-0.043000	3.031816
223.060983	3027.023649	17.378791	-0.042972	3.028088
223.020949	3019.041888	17.383795	-0.042959	3.024365
222.695958	3011.115792	17.388800	-0.042893	3.020651
222.796654	3003.106312	17.393805	-0.042907	3.016914
222.776128	2995.116084	17.398810	-0.042898	3.013175
222.737886	2987.101676	17.403815	-0.042885	3.009419
222.661263	2979.161876	17.408819	-0.042866	3.005692
222.641007	2971.180840	17.413824	-0.042857	3.001943
222.602945	2963.174502	17.418829	-0.042844	2.998177
222.539620	2955.219361	17.423834	-0.042827	2.994429
222.429474	2947.197757	17.428839	-0.042801	2.990643
222.378911	2939.200538	17.433843	-0.042787	2.986866
222.379996	2931.218530	17.438848	-0.042782	2.983094
222.192590	2923.246268	17.443853	-0.042741	2.979313
222.188306	2915.308799	17.448858	-0.042735	2.975552
222.077342	2907.292798	17.453863	-0.042709	2.971744
222.010496	2899.306710	17.458867	-0.042691	2.967948
222.187853	2891.303346	17.463872	-0.042719	2.964151
221.963048	2883.361263	17.468877	-0.042672	2.960358
221.929583	2875.411480	17.473882	-0.042661	2.956566
222.036067	2867.383610	17.478887	-0.042675	2.952739
222.119752	2859.365295	17.483891	-0.042685	2.948910
221.971227	2851.407276	17.488896	-0.042652	2.945094
221.905995	2843.427828	17.493901	-0.042635	2.941266
222.032864	2835.459374	17.498906	-0.042653	2.937449
221.791199	2827.472521	17.503911	-0.042603	2.933599
221.578973	2819.491774	17.508915	-0.042558	2.929748
221.627934	2811.525468	17.513920	-0.042562	2.925912
221.567971	2803.526535	17.518925	-0.042545	2.922050
221.520237	2795.585310	17.523930	-0.042531	2.918212
221.342512	2787.608853	17.528935	-0.042493	2.914344
221.601051	2779.476535	17.533939	-0.042536	2.910419
221.427482	2771.540361	17.538944	-0.042498	2.906561
221.413010	2763.568335	17.543949	-0.042490	2.902689
221.312576	2755.616466	17.548954	-0.042466	2.898817
221.054504	2747.672886	17.553959	-0.042413	2.894935
221.048483	2739.659005	17.558963	-0.042406	2.891027
221.091326	2731.670337	17.563968	-0.042409	2.887129
220.895934	2723.692816	17.568973	-0.042367	2.883218
220.801985	2715.759512	17.573978	-0.042344	2.879329
220.852749	2707.779432	17.578983	-0.042349	2.875419
220.811558	2699.772811	17.583987	-0.042336	2.871487
220.852090	2691.774360	17.588992	-0.042338	2.867557
220.654629	2683.811696	17.593997	-0.042296	2.863626
220.648760	2675.851794	17.599002	-0.042289	2.859702
220.569839	2667.880090	17.604007	-0.042269	2.855763
220.489854	2659.882940	17.609011	-0.042249	2.851805
220.471556	2651.892476	17.614016	-0.042240	2.847849
220.521913	2643.894014	17.619021	-0.042244	2.843887
220.502251	2635.978732	17.624026	-0.042236	2.839957
220.380173	2627.998191	17.629031	-0.042208	2.835984
220.308021	2619.993755	17.634035	-0.042189	2.831995
220.444432	2611.963692	17.639040	-0.042209	2.828001
220.134633	2604.023406	17.644045	-0.042146	2.824019
220.124466	2596.078902	17.649050	-0.042139	2.820048
220.208755	2588.067452	17.654055	-0.042149	2.816042
219.914879	2580.102709	17.659059	-0.042089	2.812032
219.847155	2572.112898	17.664064	-0.042071	2.808018
219.809490	2564.124259	17.669069	-0.042059	2.803999
219.792585	2556.181257	17.674074	-0.042050	2.799999
219.873350	2548.185101	17.679079	-0.042060	2.795973
219.877321	2540.187071	17.684083	-0.042056	2.791935
219.670249	2532.223249	17.689088	-0.042012	2.787896
219.429973	2524.251529	17.694093	-0.041962	2.783845
219.711103	2516.266521	17.699098	-0.042009	2.779812
219.677237	2508.292819	17.704103	-0.041997	2.775761
219.339949	2500.365607	17.709107	-0.041929	2.771709
219.166935	2492.379502	17.714112	-0.041891	2.767631
219.389151	2484.366282	17.719117	-0.041928	2.763557
219.390711	2476.405924	17.724122	-0.041922	2.759490
219.200546	2468.458499	17.729127	-0.041882	2.755413
219.273737	2460.380500	17.734131	-0.041890	2.751279
219.243939	2452.397275	17.739136	-0.041879	2.747180
218.952156	2444.452078	17.744141	-0.041820	2.743080
218.937390	2436.492807	17.749146	-0.041812	2.738982
218.795288	2428.529680	17.754151	-0.041780	2.734869
218.667381	2420.556379	17.759155	-0.041751	2.730745
218.661484	2412.589734	17.764160	-0.041744	2.726626
218.618226	2404.619697	17.769165	-0.041731	2.722496
218.703527	2396.641022	17.774170	-0.041742	2.718364
218.580035	2388.675355	17.779175	-0.041713	2.714219
218.688489	2380.649779	17.784179	-0.041728	2.710052
218.562897	2372.704069	17.789184	-0.041699	2.705904
218.271298	2364.743312	17.794189	-0.041640	2.701732
218.574547	2356.771224	17.799194	-0.041691	2.697585
218.598620	2348.774519	17.804199	-0.041690	2.693402
218.277984	2340.805634	17.809203	-0.041625	2.689204
218.196125	2332.868643	17.814208	-0.041605	2.685032
218.225279	2324.887287	17.819213	-0.041605	2.680837
218.309033	2316.939032	17.824218	-0.041615	2.676656
217.955406	2308.953355	17.829223	-0.041544	2.672421
217.947267	2300.949736	17.834227	-0.041537	2.668192
218.014960	2292.941905	17.839232	-0.041544	2.663959
217.801543	2285.005783	17.844237	-0.041499	2.659739
218.008631	2277.037450	17.849242	-0.041533	2.655522
217.995614	2269.027627	17.854247	-0.041525	2.651263
217.695228	2261.092563	17.859251	-0.041464	2.647017
217.750103	2253.135552	17.864256	-0.041469	2.642776
217.751652	2245.159592	17.869261	-0.041464	2.638515
217.651810	2237.210750	17.874266	-0.041440	2.634255
217.544418	2229.222210	17.879271	-0.041414	2.629966
217.368005	2221.267783	17.884275	-0.041376	2.625684
217.315847	2213.299164	17.889280	-0.041361	2.621395
217.064665	2205.333244	17.894285	-0.041309	2.617087
217.231431	2197.339397	17.899290	-0.041335	2.612786
217.278990	2189.335626	17.904295	-0.041338	2.608463
217.185597	2181.378200	17.909299	-0.041316	2.604149
216.995378	2173.445799	17.914304	-0.041275	2.599836
217.171674	2165.457632	17.919309	-0.041303	2.595509
217.155166	2157.337362	17.924314	-0.041294	2.591090
216.825835	2149.386056	17.929319	-0.041227	2.586734
216.646576	2141.466360	17.934323	-0.041189	2.582399
216.771817	2133.502687	17.939328	-0.041207	2.578053
216.595612	2125.537342	17.944333	-0.041169	2.573678
216.554037	2117.576915	17.949338	-0.041156	2.569307
216.631169	2109.611660	17.954343	-0.041165	2.564935
216.575806	2101.672157	17.959347	-0.041149	2.560560
216.510776	2093.747477	17.964352	-0.041132	2.556185
216.506640	2085.737764	17.969357	-0.041126	2.551760
216.432659	2077.784354	17.974362	-0.041107	2.547354
216.298524	2069.827640	17.979367	-0.041076	2.542933
216.282437	2061.868111	17.984371	-0.041068	2.538512
216.325880	2053.898597	17.989376	-0.041071	2.534082
215.865143	2045.949765	17.994381	-0.040980	2.529619
216.024698	2037.972724	17.999386	-0.041004	2.525177
215.893276	2030.015957	18.004391	-0.040974	2.520718
215.970921	2022.046506	18.009395	-0.040984	2.516259
215.972827	2014.039730	18.014400	-0.040979	2.511766
215.920116	2006.045985	18.019405	-0.040964	2.507267
215.771511	1998.121897	18.024410	-0.040931	2.502794
215.477454	1990.186071	18.029415	-0.040871	2.498294
215.468710	1982.228091	18.034419	-0.040864	2.493795
215.472279	1974.243770	18.039424	-0.040859	2.489274
215.414930	1966.265355	18.044429	-0.040843	2.484743
215.465079	1958.322404	18.049434	-0.040847	2.480232
215.383698	1950.372359	18.054439	-0.040827	2.475700
215.269319	1942.407591	18.059443	-0.040800	2.471147
215.265393	1934.442877	18.064448	-0.040794	2.466595
215.332282	1926.436486	18.069453	-0.040801	2.462016
215.327718	1918.519272	18.074458	-0.040795	2.457474
215.216987	1910.533996	18.079463	-0.040769	2.452877
215.090296	1902.565308	18.084467	-0.040740	2.448279
215.202176	1894.612473	18.089472	-0.040756	2.443700
215.215071	1886.654577	18.094477	-0.040753	2.439102
215.004446	1878.740601	18.099482	-0.040708	2.434503
214.773697	1870.696511	18.104487	-0.040660	2.429819
214.852456	1862.723200	18.109491	-0.040669	2.425190
214.887206	1854.782395	18.114496	-0.040671	2.420568
214.707288	1846.830134	18.119501	-0.040632	2.415914
214.883663	1838.849189	18.124506	-0.040659	2.411262
214.849740	1830.888064	18.129511	-0.040648	2.406596
214.611845	1822.961851	18.134515	-0.040598	2.401926
214.442228	1815.038114	18.139520	-0.040561	2.397253
214.539894	1807.048436	18.144525	-0.040574	2.392554
214.556606	1799.085213	18.149530	-0.040572	2.387854
214.461555	1791.107536	18.154535	-0.040549	2.383127
214.333303	1783.188081	18.159539	-0.040520	2.378424
214.317023	1775.249630	18.164544	-0.040512	2.373708
214.081226	1767.270789	18.169549	-0.040462	2.368941
214.050908	1759.327548	18.174554	-0.040451	2.364203
213.917502	1751.383611	18.179559	-0.040421	2.359446
213.617695	1743.466532	18.184563	-0.040360	2.354682
213.995113	1735.403846	18.189568	-0.040425	2.349876
213.596783	1727.487925	18.194573	-0.040346	2.345085
213.426502	1719.559303	18.199578	-0.040309	2.340296
213.603812	1711.580667	18.204583	-0.040336	2.335494
213.752151	1703.585640	18.209587	-0.040359	2.330671
213.680714	1695.635199	18.214592	-0.040340	2.325847
213.239534	1687.742499	18.219597	-0.040253	2.321017
213.542429	1679.770221	18.224602	-0.040304	2.316190
213.447683	1671.806371	18.229607	-0.040281	2.311325
213.259625	1663.851969	18.234611	-0.040241	2.306448
213.275517	1655.917330	18.239616	-0.040238	2.301589
213.177771	1647.968542	18.244621	-0.040215	2.296703
213.159869	1640.003177	18.249626	-0.040206	2.291802
213.078456	1632.047410	18.254631	-0.040186	2.286891
213.142627	1624.099036	18.259635	-0.040192	2.281987
213.046475	1616.177756	18.264640	-0.040169	2.277075
212.931596	1608.176177	18.269645	-0.040143	2.272101
212.926058	1600.185311	18.274650	-0.040136	2.267132
212.895409	1592.246718	18.279655	-0.040125	2.262183
212.776586	1584.316784	18.284659	-0.040098	2.257220
212.747446	1576.377678	18.289664	-0.040087	2.252249
212.702216	1568.413355	18.294669	-0.040073	2.247249
212.723399	1560.493968	18.299674	-0.040072	2.242273
212.481126	1552.579941	18.304679	-0.040022	2.237265
212.543759	1544.603349	18.309683	-0.040028	2.232234
212.460527	1536.654278	18.314688	-0.040007	2.227196
212.156905	1528.723185	18.319693	-0.039945	2.222138
212.315863	1520.774549	18.324698	-0.039970	2.217098
212.248024	1512.821442	18.329703	-0.039952	2.212024
212.038270	1504.886589	18.334707	-0.039908	2.206937
211.931328	1496.952982	18.339712	-0.039882	2.201849
212.049171	1488.995818	18.344717	-0.039899	2.196754
212.109219	1481.024220	18.349722	-0.039905	2.191632
211.638633	1473.108623	18.354727	-0.039812	2.186486
211.675129	1465.162986	18.359731	-0.039813	2.181355
211.582015	1457.230578	18.364736	-0.039791	2.176209
211.602092	1449.260302	18.369741	-0.039789	2.171036
211.629764	1441.317012	18.374746	-0.039789	2.165869
211.445596	1433.403968	18.379751	-0.039750	2.160690
211.361042	1425.488397	18.384755	-0.039729	2.155506
211.527828	1417.488665	18.389760	-0.039754	2.150278
211.530106	1409.536548	18.394765	-0.039749	2.145052
211.327346	1401.650697	18.399770	-0.039706	2.139839
211.326756	1393.702048	18.404775	-0.039701	2.134590
211.362051	1385.740450	18.409779	-0.039702	2.129323
211.313774	1377.823223	18.414784	-0.039688	2.124065
210.938217	1369.939040	18.419789	-0.039613	2.118784
210.903404	1361.981413	18.424794	-0.039601	2.113474
211.045702	1353.953605	18.429799	-0.039622	2.108120
210.949408	1346.031526	18.434803	-0.039599	2.102801
210.832584	1338.129272	18.439808	-0.039572	2.097479
210.704976	1330.197794	18.444813	-0.039543	2.092123
210.674858	1322.260998	18.449818	-0.039532	2.086759
210.635841	1314.325646	18.454823	-0.039520	2.081382
210.583110	1306.412577	18.459827	-0.039505	2.076004
210.431563	1298.487035	18.464832	-0.039471	2.070594
210.363492	1290.536531	18.469837	-0.039453	2.065161
210.405051	1282.611450	18.474842	-0.039456	2.059742
210.237078	1274.708313	18.479847	-0.039419	2.054303
210.297049	1266.736137	18.484851	-0.039425	2.048825
210.210330	1258.832968	18.489856	-0.039404	2.043365
210.223704	1250.891622	18.494861	-0.039401	2.037874
210.031656	1242.984124	18.499866	-0.039360	2.032371
209.579126	1235.074464	18.504871	-0.039270	2.026824
209.751842	1227.117093	18.509875	-0.039297	2.021293
210.024244	1219.166833	18.514880	-0.039343	2.015763
209.622717	1211.262496	18.519885	-0.039262	2.010179
209.611744	1203.346276	18.524890	-0.039255	2.004612
209.589252	1195.427426	18.529895	-0.039246	1.999027
209.504514	1187.508416	18.534899	-0.039225	1.993419
209.346352	1179.594070	18.539904	-0.039190	1.987791
209.415129	1171.643450	18.544909	-0.039197	1.982145
209.551782	1163.719925	18.549914	-0.039218	1.976510
209.365022	1155.802624	18.554919	-0.039178	1.970828
209.168526	1147.901038	18.559923	-0.039136	1.965141
209.405030	1139.974984	18.564928	-0.039175	1.959465
209.268021	1132.061313	18.569933	-0.039144	1.953742
209.189001	1124.110287	18.574938	-0.039124	1.947981
208.997154	1116.205356	18.579943	-0.039083	1.942224
208.972685	1108.286599	18.584947	-0.039073	1.936459
208.843732	1100.376408	18.589952	-0.039044	1.930670
208.735816	1092.451501	18.594957	-0.039018	1.924856
208.717792	1084.566099	18.599962	-0.039010	1.919064
208.494595	1076.666109	18.604967	-0.038963	1.913220
208.277368	1068.763138	18.609971	-0.038917	1.907356
208.406164	1060.823962	18.614976	-0.038936	1.901487
208.216466	1052.926472	18.619981	-0.038895	1.895594
208.252709	1045.004489	18.624986	-0.038897	1.889690
208.189995	1037.095589	18.629991	-0.038880	1.883767
208.236192	1029.192498	18.634995	-0.038883	1.877841
208.284842	1021.270013	18.640000	-0.038887	1.871882
207.978692	1013.372597	18.645005	-0.038825	1.865883
208.093275	1005.456008	18.650010	-0.038841	1.859898
208.010841	997.567458	18.655015	-0.038820	1.853892
207.866321	989.655166	18.660019	-0.038788	1.847841
208.010976	981.743228	18.665024	-0.038810	1.841805
207.683707	973.884118	18.670029	-0.038744	1.835734
207.673965	965.982970	18.675034	-0.038737	1.829647
207.714606	958.058169	18.680039	-0.038739	1.823528
207.619864	950.182785	18.685043	-0.038716	1.817411
207.526576	942.292872	18.690048	-0.038693	1.811262
207.225777	934.415773	18.695053	-0.038632	1.805076
207.528473	926.500509	18.700058	-0.038683	1.798913
207.280290	918.605859	18.705063	-0.038632	1.792678
207.075243	910.688504	18.710067	-0.038588	1.786408
207.200111	902.782662	18.715072	-0.038606	1.780165
207.124593	894.897903	18.720077	-0.038587	1.773893
207.121240	886.997558	18.725082	-0.038581	1.767595
206.842433	879.150959	18.730087	-0.038524	1.761283
206.937175	871.259611	18.735091	-0.038536	1.754959
206.944871	863.364735	18.740096	-0.038533	1.748599
206.623318	855.515587	18.745101	-0.038467	1.742211
206.679571	847.632617	18.750106	-0.038473	1.735819
206.633900	839.738152	18.755111	-0.038459	1.729382
206.327673	831.896485	18.760115	-0.038397	1.722930
206.172408	824.052523	18.765120	-0.038363	1.716472
206.222288	816.115478	18.770125	-0.038367	1.709938
206.173642	808.236444	18.775130	-0.038352	1.703415
206.092598	800.365864	18.780135	-0.038332	1.696870
206.080587	792.473078	18.785139	-0.038324	1.690290
206.001651	784.617849	18.790144	-0.038305	1.683707
205.891657	776.758966	18.795149	-0.038279	1.677091
205.924405	768.881161	18.800154	-0.038280	1.670451
205.845067	761.009885	18.805159	-0.038260	1.663776
205.575980	753.189399	18.810163	-0.038204	1.657091
205.753376	745.279587	18.815168	-0.038232	1.650363
205.600820	737.440385	18.820173	-0.038199	1.643624
205.363672	729.626294	18.825178	-0.038149	1.636866
205.155996	721.726561	18.830183	-0.038105	1.630011
205.355917	713.807390	18.835187	-0.038137	1.623166
205.494523	705.943498	18.840192	-0.038158	1.616332
205.198423	698.116329	18.845197	-0.038097	1.609440
204.942739	690.309886	18.850202	-0.038045	1.602542
205.161392	682.424310	18.855207	-0.038080	1.595612
205.128842	674.568489	18.860211	-0.038069	1.588642
204.923926	666.752314	18.865216	-0.038025	1.581652
204.769668	658.931499	18.870221	-0.037992	1.574634
204.949491	651.050606	18.875226	-0.038020	1.567579
204.594282	643.262259	18.880231	-0.037948	1.560498
204.509932	635.434471	18.885235	-0.037928	1.553388
204.599906	627.554266	18.890240	-0.037939	1.546223
204.439022	619.736466	18.895245	-0.037904	1.539045
204.369987	611.911858	18.900250	-0.037886	1.531841
204.230836	604.086058	18.905255	-0.037855	1.524591
204.196263	596.269453	18.910259	-0.037843	1.517331
204.212373	588.433526	18.915264	-0.037841	1.510026
204.211708	580.603584	18.920269	-0.037836	1.502688
204.138356	572.806972	18.925274	-0.037817	1.495334
203.840389	565.011901	18.930279	-0.037756	1.487910
204.000126	557.166137	18.935283	-0.037781	1.480473
203.987097	549.354444	18.940288	-0.037773	1.473003
203.600920	541.547770	18.945293	-0.037696	1.465441
203.569487	533.758608	18.950298	-0.037685	1.457913
203.792975	525.895021	18.955303	-0.037721	1.450315
203.480607	518.153502	18.960307	-0.037658	1.442709
203.365312	510.383139	18.965312	-0.037631	1.435067
203.297133	502.568297	18.970317	-0.037613	1.427347
203.450103	494.754915	18.975322	-0.037637	1.419623
203.295087	486.989587	18.980327	-0.037603	1.411854
203.216342	479.207094	18.985331	-0.037583	1.404038
203.135361	471.457022	18.990336	-0.037563	1.396210
202.846326	463.688379	18.995341	-0.037504	1.388284
202.719061	455.928615	19.000346	-0.037475	1.380348
202.661377	448.150491	19.005351	-0.037459	1.372360
202.487780	440.394517	19.010355	-0.037421	1.364328
202.329104	432.664580	19.015360	-0.037387	1.356278
202.254057	424.884513	19.020365	-0.037367	1.348142
202.244456	417.130061	19.025370	-0.037360	1.339996
202.128419	409.380954	19.030375	-0.037334	1.331786
202.065160	401.635020	19.035379	-0.037317	1.323538
202.122214	393.878738	19.040384	-0.037322	1.315248
201.979886	386.017539	19.045389	-0.037291	1.306757
201.921507	378.311008	19.050394	-0.037275	1.298393
201.960830	370.575497	19.055399	-0.037277	1.289962
201.829586	362.874649	19.060403	-0.037247	1.281482
201.580696	355.208185	19.065408	-0.037196	1.272961
201.399593	347.497086	19.070413	-0.037157	1.264345
201.436283	339.788152	19.075418	-0.037159	1.255715
201.294217	332.095489	19.080423	-0.037127	1.247008
201.123849	324.431046	19.085427	-0.037090	1.238267
201.196757	316.711094	19.090432	-0.037099	1.229448
201.037541	309.026784	19.095437	-0.037064	1.220560
200.817748	301.385409	19.100442	-0.037018	1.211646
200.869340	293.688886	19.105447	-0.037022	1.202654
200.871538	286.021409	19.110451	-0.037018	1.193619
200.575970	278.397632	19.115456	-0.036958	1.184507
200.435211	270.758214	19.120461	-0.036926	1.175337
200.490634	263.086102	19.125466	-0.036931	1.166096
200.358619	255.478391	19.130471	-0.036902	1.156820
200.323258	247.789464	19.135475	-0.036890	1.147390
200.200675	240.189129	19.140480	-0.036862	1.137973
199.856818	232.604289	19.145485	-0.036793	1.128449
199.969407	224.980732	19.150490	-0.036809	1.118894
199.741744	217.402136	19.155495	-0.036762	1.109240
199.779326	209.793899	19.160499	-0.036764	1.099521
199.316051	202.282007	19.165504	-0.036672	1.089729
199.212665	194.705619	19.170509	-0.036648	1.079844
199.052990	187.156152	19.175514	-0.036613	1.069891
198.838625	179.610735	19.180519	-0.036568	1.059837
198.451066	172.116662	19.185523	-0.036491	1.049715
198.130519	164.620076	19.190528	-0.036426	1.039507
197.762417	157.132100	19.195533	-0.036353	1.029198
197.619720	149.623518	19.200538	-0.036321	1.018810
197.250244	142.161383	19.205543	-0.036248	1.008325
196.833383	134.723391	19.210547	-0.036165	0.997752
196.376196	127.261046	19.215552	-0.036075	0.987021
195.975443	119.827909	19.220557	-0.035995	0.976228
195.711900	112.388163	19.225562	-0.035941	0.965339
195.177031	105.020435	19.230567	-0.035837	0.954363
194.506528	97.669302	19.235571	-0.035707	0.943247
194.213214	90.277335	19.240576	-0.035648	0.932037
193.672063	82.938259	19.245581	-0.035542	0.920705
193.267320	75.593420	19.250586	-0.035462	0.909260
192.792399	68.268678	19.255591	-0.035368	0.897680
192.279965	61.197788	19.260595	-0.035268	0.886343