Thu Mar 11 19:56:19 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.378392	0.005779	0.000000	0.000023	0.719412

0.514548	0.006049	0.005005	-0.000002	0.719461
0.466445	-0.082408	0.010010	0.000007	0.719269
0.366805	-0.059341	0.015014	0.000026	0.719279
0.403534	-0.069940	0.020019	0.000019	0.719271
0.650438	-0.113894	0.025024	-0.000027	0.719271
0.634657	-0.109008	0.030029	-0.000024	0.719275
0.378078	-0.065825	0.035034	0.000024	0.719270
0.432124	-0.068982	0.040038	0.000014	0.719282
0.494997	-0.085583	0.045043	0.000002	0.719271
0.405421	-0.067078	0.050048	0.000019	0.719276
0.464254	-0.076747	0.055053	0.000008	0.719278
0.383322	-0.066469	0.060058	0.000024	0.719269
0.361961	-0.055840	0.065062	0.000028	0.719283
0.331055	-0.055066	0.070067	0.000033	0.719273
0.430269	-0.072678	0.075072	0.000015	0.719273
0.400252	-0.184585	0.080077	0.000021	0.719042
0.233351	-0.195980	0.085082	0.000052	0.718960
0.285622	-0.199931	0.090086	0.000042	0.718971
0.222099	-0.192475	0.095091	0.000054	0.718963
-0.004458	-0.150841	0.100096	0.000097	0.718965
0.100734	-0.167263	0.105101	0.000077	0.718969
0.224745	-0.192377	0.110106	0.000054	0.718963
0.450777	-0.341492	0.115110	0.000012	0.718748
0.341800	-0.373624	0.120115	0.000033	0.718646
0.499116	-0.400636	0.125120	0.000004	0.718648
0.527210	-0.404989	0.130125	-0.000002	0.718649
0.267971	-0.361487	0.135130	0.000047	0.718644
0.416599	-0.499180	0.140134	0.000019	0.718424
0.461129	-0.542663	0.145139	0.000011	0.718354
0.331876	-0.518872	0.150144	0.000035	0.718355
0.330198	-0.514603	0.155149	0.000036	0.718363
0.261095	-0.605373	0.160154	0.000049	0.718159
0.386328	-0.694308	0.165158	0.000026	0.718027
0.317259	-0.685384	0.170163	0.000038	0.718020
0.223036	-0.667082	0.175168	0.000056	0.718023
0.255809	-0.802328	0.180173	0.000050	0.717767
0.242960	-0.829478	0.185178	0.000053	0.717709
0.283813	-0.834762	0.190182	0.000045	0.717712
0.408074	-0.929325	0.195187	0.000022	0.717569
0.293807	-1.002977	0.200192	0.000044	0.717383
0.184137	-0.980266	0.205197	0.000064	0.717389
0.115804	-1.013185	0.210202	0.000077	0.717300
0.168142	-1.124288	0.215206	0.000067	0.717098
0.052943	-1.108444	0.220211	0.000089	0.717089
-0.063608	-1.134017	0.225216	0.000111	0.716997
0.036485	-1.268056	0.230221	0.000092	0.716767
0.032702	-1.272174	0.235226	0.000093	0.716757
-0.017679	-1.325795	0.240230	0.000103	0.716633
-0.121413	-1.397848	0.245235	0.000122	0.716453
-0.078971	-1.404246	0.250240	0.000114	0.716456
-0.112339	-1.511351	0.255245	0.000121	0.716231
-0.272670	-1.532338	0.260250	0.000151	0.716133
0.011647	-1.596282	0.265254	0.000098	0.716107
-0.089190	-1.688634	0.270259	0.000117	0.715888
0.009462	-1.704850	0.275264	0.000099	0.715890
0.114632	-1.843002	0.280269	0.000079	0.715653
-0.137672	-1.849846	0.285274	0.000126	0.715551
-0.101441	-1.918554	0.290278	0.000120	0.715427
0.163831	-2.062525	0.295283	0.000070	0.715235
-0.069975	-2.054063	0.300288	0.000114	0.715169
-0.260222	-2.145091	0.305293	0.000150	0.714921
-0.305330	-2.145374	0.310298	0.000158	0.714904
-0.299393	-2.290726	0.315302	0.000157	0.714617
-0.650317	-2.232278	0.320307	0.000223	0.714609
-1.123086	-2.286979	0.325312	0.000311	0.714333
-2.880240	-1.998862	0.330317	0.000638	0.714283
-2.392931	-2.113637	0.335322	0.000547	0.714228
-2.797271	-2.168076	0.340326	0.000623	0.713976
-3.357732	-2.069343	0.345331	0.000727	0.713974
-3.410388	-2.076320	0.350336	0.000737	0.713941
-3.751759	-2.157351	0.355341	0.000801	0.713659
-4.353764	-2.053137	0.360346	0.000913	0.713653
-4.328129	-2.052817	0.365350	0.000908	0.713662
-4.181741	-2.177366	0.370355	0.000881	0.713466
-5.332090	-2.022701	0.375360	0.001095	0.713366
-5.103419	-2.061423	0.380365	0.001053	0.713370
-4.866765	-2.108081	0.385370	0.001009	0.713361
-5.499095	-2.148876	0.390374	0.001127	0.713055
-6.205818	-2.035253	0.395379	0.001259	0.713031
-6.247608	-2.029239	0.400384	0.001266	0.713028
-5.675815	-2.128432	0.405389	0.001160	0.713033
-6.632248	-2.067922	0.410394	0.001338	0.712814
-7.441448	-1.972415	0.415398	0.001489	0.712717
-6.824921	-2.082954	0.420403	0.001374	0.712715
-6.929029	-2.065953	0.425408	0.001394	0.712712
-7.200965	-2.014070	0.430413	0.001445	0.712718
-7.126460	-2.142880	0.435418	0.001431	0.712488
-7.841970	-2.060906	0.440422	0.001564	0.712397
-8.008345	-2.034808	0.445427	0.001595	0.712390
-7.928998	-2.049005	0.450432	0.001581	0.712390
-7.816838	-2.066737	0.455437	0.001560	0.712394
-8.050640	-2.103577	0.460442	0.001603	0.712238
-9.041037	-1.998768	0.465446	0.001788	0.712095
-8.590325	-2.079686	0.470451	0.001704	0.712093
-8.821548	-2.038153	0.475456	0.001747	0.712094
-8.868045	-2.027224	0.480461	0.001756	0.712099
-9.072972	-1.993980	0.485466	0.001794	0.712092
-9.039352	-2.107098	0.490470	0.001788	0.711878
-10.265561	-1.946995	0.495475	0.002016	0.711762
-10.040142	-1.984520	0.500480	0.001975	0.711767
-9.439272	-2.088438	0.505485	0.001863	0.711773
-10.117759	-1.973313	0.510490	0.001989	0.711761
-10.033080	-1.984116	0.515494	0.001974	0.711769
-9.569198	-2.097330	0.520499	0.001887	0.711708
-10.694096	-2.021792	0.525504	0.002097	0.711459
-10.667493	-2.023031	0.530509	0.002092	0.711466
-11.130068	-1.944770	0.535514	0.002178	0.711457
-10.685010	-2.020301	0.540518	0.002096	0.711465
-10.599831	-2.038434	0.545523	0.002080	0.711459
-10.902471	-1.983742	0.550528	0.002136	0.711460
-10.752654	-2.097124	0.555533	0.002108	0.711287
-12.089011	-1.931179	0.560538	0.002357	0.711143
-11.755259	-1.985510	0.565542	0.002295	0.711153
-11.278633	-2.075040	0.570547	0.002207	0.711143
-11.676290	-2.003885	0.575552	0.002281	0.711144
-11.600112	-2.015484	0.580557	0.002267	0.711147
-11.775985	-1.987097	0.585562	0.002300	0.711141
-11.754697	-2.091963	0.590566	0.002296	0.710939
-12.627458	-1.967462	0.595571	0.002458	0.710877
-12.781722	-1.941282	0.600576	0.002487	0.710874
-12.056856	-2.065743	0.605581	0.002352	0.710884
-12.583179	-1.976858	0.610586	0.002450	0.710874
-12.635095	-1.965046	0.615590	0.002460	0.710879
-12.315643	-2.037514	0.620595	0.002401	0.710847
-13.136288	-2.047756	0.625600	0.002554	0.710535
-13.102273	-2.050125	0.630605	0.002547	0.710542
-13.792534	-1.931748	0.635610	0.002676	0.710532
-13.104272	-2.049027	0.640614	0.002548	0.710543
-13.107635	-2.050870	0.645619	0.002549	0.710538
-13.587768	-1.965444	0.650624	0.002638	0.710537
-13.186735	-2.094878	0.655629	0.002564	0.710421
-14.249009	-2.008256	0.660634	0.002762	0.710216
-14.018797	-2.043638	0.665638	0.002719	0.710227
-14.119487	-2.029190	0.670643	0.002738	0.710220
-14.527821	-1.956909	0.675648	0.002814	0.710219
-14.257160	-2.002038	0.680653	0.002764	0.710225
-14.389209	-1.982353	0.685658	0.002788	0.710217
-13.988119	-2.136335	0.690662	0.002714	0.710052
-15.228676	-1.991880	0.695667	0.002945	0.709899
-15.263597	-1.987277	0.700672	0.002951	0.709895
-14.793680	-2.068387	0.705677	0.002864	0.709900
-15.023805	-2.029269	0.710682	0.002907	0.709896
-15.230964	-1.989012	0.715686	0.002946	0.709903
-15.239496	-1.991142	0.720691	0.002947	0.709895
-15.312847	-2.077161	0.725696	0.002961	0.709697
-15.881349	-2.022969	0.730701	0.003067	0.709602
-16.401926	-1.933803	0.735706	0.003164	0.709595
-15.933864	-2.013766	0.740710	0.003077	0.709602
-15.806420	-2.036420	0.745715	0.003053	0.709602
-16.038408	-1.995525	0.750720	0.003097	0.709601
-16.002820	-2.000794	0.755725	0.003090	0.709602
-16.123831	-2.090214	0.760730	0.003113	0.709380
-16.989400	-1.988905	0.765734	0.003274	0.709274
-16.609677	-2.059251	0.770739	0.003203	0.709269
-16.730639	-2.038064	0.775744	0.003226	0.709268
-16.876089	-2.009547	0.780749	0.003253	0.709273
-17.154738	-1.963182	0.785754	0.003305	0.709266
-16.433609	-2.086339	0.790758	0.003171	0.709276
-17.108105	-2.103888	0.795763	0.003297	0.709000
-18.398645	-1.892771	0.800768	0.003537	0.708962
-17.850816	-1.987698	0.805773	0.003435	0.708968
-17.489360	-2.056778	0.810778	0.003368	0.708958
-17.792023	-1.998410	0.815782	0.003424	0.708967
-18.131355	-1.939745	0.820787	0.003488	0.708963
-17.725435	-2.012344	0.825792	0.003412	0.708962
-17.524288	-2.139860	0.830797	0.003375	0.708779
-18.908429	-1.960453	0.835802	0.003633	0.708644
-18.786423	-1.978983	0.840806	0.003610	0.708650
-18.477711	-2.034959	0.845811	0.003553	0.708648
-18.672846	-2.001758	0.850816	0.003589	0.708644
-18.466531	-2.035237	0.855821	0.003551	0.708651
-18.523361	-2.030349	0.860826	0.003562	0.708640
-18.701950	-2.101634	0.865830	0.003595	0.708433
-19.715306	-1.957931	0.870835	0.003784	0.708359
-19.515181	-1.995683	0.875840	0.003747	0.708355
-19.365214	-2.017134	0.880845	0.003719	0.708365
-19.735329	-1.955666	0.885850	0.003788	0.708356
-19.203985	-2.047622	0.890854	0.003689	0.708361
-19.015258	-2.081162	0.895859	0.003654	0.708361
-20.187746	-2.036427	0.900864	0.003872	0.708032
-20.506567	-1.982852	0.905869	0.003932	0.708025
-20.483437	-1.990770	0.910874	0.003928	0.708017
-20.132862	-2.049148	0.915878	0.003862	0.708025
-20.722165	-1.945611	0.920883	0.003972	0.708022
-20.647576	-1.961845	0.925888	0.003958	0.708016
-19.780039	-2.111897	0.930893	0.003797	0.708025
-20.709907	-2.077631	0.935898	0.003970	0.707761
-21.643379	-1.937186	0.940902	0.004144	0.707709
-20.922466	-2.066907	0.945907	0.004010	0.707706
-21.087379	-2.037143	0.950912	0.004041	0.707707
-21.549010	-1.951884	0.955917	0.004127	0.707713
-21.329157	-1.995448	0.960922	0.004086	0.707704
-20.997412	-2.051835	0.965926	0.004024	0.707709
-21.728185	-2.050462	0.970931	0.004161	0.707450
-22.518642	-1.945061	0.975936	0.004308	0.707379
-21.992741	-2.033335	0.980941	0.004210	0.707390
-22.281015	-1.986988	0.985946	0.004264	0.707379
-22.344302	-1.972926	0.990950	0.004276	0.707385
-21.993827	-2.036349	0.995955	0.004211	0.707383
-22.261513	-1.990677	1.000960	0.004260	0.707378
-22.436627	-2.026493	1.005965	0.004293	0.707244
-23.030331	-2.002691	1.010970	0.004404	0.707079
-22.498001	-2.092038	1.015974	0.004305	0.707090
-22.966914	-2.009640	1.020979	0.004392	0.707087
-23.332318	-1.945032	1.025984	0.004460	0.707086
-22.629827	-2.067819	1.030989	0.004330	0.707091
-22.972316	-2.011728	1.035994	0.004394	0.707081
-23.776025	-1.983547	1.040998	0.004543	0.706849
-23.947162	-1.998257	1.046003	0.004575	0.706758
-23.795403	-2.027543	1.051008	0.004547	0.706754
-24.021444	-1.982606	1.056013	0.004589	0.706763
-24.595245	-1.884462	1.061018	0.004696	0.706754
-24.031540	-1.981854	1.066022	0.004591	0.706760
-23.712645	-2.039261	1.071027	0.004532	0.706759
-24.103457	-1.996546	1.076032	0.004605	0.706705
-24.515324	-2.048633	1.081037	0.004682	0.706452
-24.601115	-2.037631	1.086042	0.004698	0.706443
-25.155855	-1.935230	1.091046	0.004801	0.706450
-24.754388	-2.007046	1.096051	0.004727	0.706450
-24.909088	-1.980848	1.101056	0.004755	0.706447
-24.909498	-1.977570	1.106061	0.004756	0.706453
-24.873852	-2.006276	1.111066	0.004749	0.706408
-25.045915	-2.109867	1.116070	0.004781	0.706138
-25.412289	-2.046013	1.121075	0.004850	0.706135
-26.172032	-1.912502	1.126080	0.004991	0.706130
-25.138976	-2.091743	1.131085	0.004799	0.706140
-25.255846	-2.076558	1.136090	0.004821	0.706129
-25.811142	-1.974600	1.141094	0.004924	0.706134
-25.671138	-2.078962	1.146099	0.004898	0.705975
-26.322963	-2.016773	1.151104	0.005020	0.705866
-26.266275	-2.021269	1.156109	0.005009	0.705877
-26.592584	-1.969018	1.161114	0.005070	0.705865
-26.394656	-2.001332	1.166118	0.005033	0.705871
-26.342383	-2.010436	1.171123	0.005024	0.705871
-26.620184	-1.962369	1.176128	0.005076	0.705868
-26.872366	-2.075270	1.181133	0.005123	0.705550
-27.195308	-2.027455	1.186138	0.005183	0.705530
-27.526296	-1.966064	1.191142	0.005245	0.705535
-27.173748	-2.028271	1.196147	0.005179	0.705536
-27.235583	-2.021340	1.201152	0.005191	0.705527
-27.186212	-2.023953	1.206157	0.005182	0.705540
-27.184421	-2.064553	1.211162	0.005181	0.705458
-27.781228	-2.076764	1.216166	0.005293	0.705219
-27.780401	-2.076969	1.221171	0.005293	0.705219
-28.666470	-1.920616	1.226176	0.005458	0.705216
-28.058821	-2.025394	1.231181	0.005345	0.705223
-27.861144	-2.066469	1.236186	0.005308	0.705211
-28.280475	-1.986499	1.241190	0.005386	0.705221
-28.253917	-2.075958	1.246195	0.005381	0.705050
-29.075986	-2.008720	1.251200	0.005534	0.704890
-28.531143	-2.100832	1.256205	0.005433	0.704900
-29.174350	-1.988663	1.261210	0.005553	0.704895
-29.223769	-1.979213	1.266214	0.005562	0.704896
-28.745049	-2.063452	1.271219	0.005473	0.704898
-29.163780	-1.991107	1.276224	0.005551	0.704893
-29.417000	-2.047693	1.281229	0.005599	0.704688
-30.031972	-1.984174	1.286234	0.005713	0.704595
-29.950665	-1.996170	1.291238	0.005698	0.704600
-29.900941	-2.005014	1.296243	0.005689	0.704600
-29.906994	-2.007014	1.301248	0.005690	0.704593
-29.915970	-2.001249	1.306253	0.005692	0.704601
-29.895106	-2.009248	1.311258	0.005688	0.704593
-29.965833	-2.096658	1.316262	0.005701	0.704391
-30.825647	-2.002280	1.321267	0.005862	0.704272
-31.097204	-1.957640	1.326272	0.005912	0.704264
-30.677938	-2.027877	1.331277	0.005834	0.704273
-30.508754	-2.061581	1.336282	0.005803	0.704266
-30.583706	-2.046843	1.341286	0.005817	0.704268
-30.793367	-2.010063	1.346291	0.005856	0.704267
-31.146025	-2.066280	1.351296	0.005922	0.704027
-31.440341	-2.044129	1.356301	0.005977	0.703965
-31.865822	-1.971618	1.361306	0.006056	0.703958
-31.843931	-1.972985	1.366310	0.006052	0.703963
-31.490338	-2.035386	1.371315	0.005986	0.703964
-31.595443	-2.019143	1.376320	0.006006	0.703959
-31.553688	-2.022735	1.381325	0.005998	0.703967
-32.190501	-2.031834	1.386330	0.006117	0.703719
-32.897869	-1.942677	1.391334	0.006249	0.703644
-32.683387	-1.978731	1.396339	0.006209	0.703648
-32.698579	-1.981998	1.401344	0.006212	0.703636
-32.641923	-1.987669	1.406349	0.006202	0.703645
-32.704385	-1.980496	1.411354	0.006213	0.703637
-32.479786	-2.018702	1.416358	0.006172	0.703640
-32.575409	-2.044720	1.421363	0.006189	0.703553
-33.638547	-1.958320	1.426368	0.006387	0.703345
-33.362646	-2.002890	1.431373	0.006336	0.703354
-33.266459	-2.022223	1.436378	0.006318	0.703349
-33.490406	-1.983357	1.441382	0.006360	0.703347
-33.701057	-1.946320	1.446387	0.006400	0.703346
-33.725908	-1.942680	1.451392	0.006404	0.703344
-33.189391	-2.078410	1.456397	0.006305	0.703263
-34.336496	-2.000178	1.461402	0.006518	0.703008
-34.417905	-1.982667	1.466406	0.006533	0.703013
-34.462786	-1.972132	1.471411	0.006542	0.703018
-34.432388	-1.982517	1.476416	0.006536	0.703008
-34.273460	-2.005230	1.481421	0.006507	0.703019
-34.234199	-2.017002	1.486426	0.006500	0.703010
-34.252156	-2.047823	1.491430	0.006503	0.702941
-34.931813	-2.042907	1.496435	0.006630	0.702705
-35.207427	-1.996409	1.501440	0.006681	0.702700
-35.221044	-1.989326	1.506445	0.006684	0.702709
-35.346702	-1.971033	1.511450	0.006707	0.702701
-35.375605	-1.964237	1.516454	0.006713	0.702704
-34.944802	-2.040798	1.521459	0.006633	0.702704
-35.142560	-2.058161	1.526464	0.006670	0.702598
-36.165480	-1.979545	1.531469	0.006860	0.702388
-35.801396	-2.049114	1.536474	0.006793	0.702378
-35.975051	-2.016122	1.541478	0.006825	0.702382
-36.369478	-1.946391	1.546483	0.006898	0.702380
-36.198425	-1.979843	1.551488	0.006867	0.702374
-35.749842	-2.055908	1.556493	0.006783	0.702382
-36.218441	-2.028658	1.561498	0.006871	0.702268
-37.195982	-1.945960	1.566502	0.007053	0.702083
-36.660588	-2.039863	1.571507	0.006953	0.702086
-36.878488	-2.004384	1.576512	0.006994	0.702079
-36.948425	-1.987764	1.581517	0.007007	0.702087
-36.829375	-2.012367	1.586522	0.006985	0.702080
-36.793628	-2.017409	1.591526	0.006978	0.702082
-36.958269	-2.079595	1.596531	0.007009	0.701897
-38.130554	-1.944143	1.601536	0.007227	0.701748
-37.683416	-2.017952	1.606541	0.007144	0.701760
-37.930938	-1.978308	1.611546	0.007191	0.701750
-38.160295	-1.936773	1.616550	0.007233	0.701751
-37.495991	-2.054088	1.621555	0.007110	0.701753
-37.647594	-2.029504	1.626560	0.007138	0.701748
-38.052018	-2.034657	1.631565	0.007214	0.701592
-38.753498	-1.982889	1.636570	0.007344	0.701443
-38.354997	-2.051075	1.641574	0.007270	0.701449
-38.742646	-1.981891	1.646579	0.007342	0.701449
-39.303071	-1.885136	1.651584	0.007447	0.701442
-38.393603	-2.041854	1.656589	0.007278	0.701453
-38.670917	-1.996316	1.661594	0.007329	0.701445
-39.108377	-1.988218	1.666598	0.007411	0.701303
-39.830902	-1.943568	1.671603	0.007546	0.701132
-39.531008	-2.000917	1.676608	0.007490	0.701124
-39.736819	-1.957568	1.681613	0.007528	0.701138
-39.649391	-1.978070	1.686618	0.007512	0.701127
-39.546949	-1.995469	1.691622	0.007493	0.701129
-39.677780	-1.970770	1.696627	0.007518	0.701132
-39.801841	-1.962268	1.701632	0.007541	0.701104
-40.047401	-2.025798	1.706637	0.007587	0.700886
-40.407826	-1.965857	1.711642	0.007654	0.700877
-40.467795	-1.953294	1.716646	0.007665	0.700881
-39.844618	-2.061589	1.721651	0.007549	0.700886
-40.377203	-1.970678	1.726656	0.007648	0.700878
-40.386757	-1.966142	1.731661	0.007650	0.700883
-40.539933	-2.030090	1.736666	0.007679	0.700698
-41.152733	-1.998458	1.741670	0.007793	0.700541
-40.875192	-2.046738	1.746675	0.007742	0.700543
-41.297882	-1.974265	1.751680	0.007820	0.700537
-41.049572	-2.012904	1.756685	0.007774	0.700548
-40.863513	-2.050645	1.761690	0.007740	0.700539
-41.221150	-2.020111	1.766694	0.007806	0.700471
-42.090074	-1.985996	1.771699	0.007968	0.700226
-42.085626	-1.990656	1.776704	0.007968	0.700218
-42.194747	-1.965364	1.781709	0.007988	0.700229
-42.228090	-1.962476	1.786714	0.007994	0.700223
-42.000953	-2.001614	1.791718	0.007952	0.700226
-42.100624	-1.982010	1.796723	0.007971	0.700229
-42.399206	-1.941326	1.801728	0.008026	0.700203
-42.747184	-2.026566	1.806733	0.008091	0.699904
-42.977712	-1.987357	1.811738	0.008134	0.699900
-43.416588	-1.908876	1.816742	0.008216	0.699901
-42.701317	-2.034222	1.821747	0.008083	0.699905
-43.012454	-1.982484	1.826752	0.008141	0.699897
-43.217760	-1.939425	1.831757	0.008179	0.699910
-43.272516	-1.931909	1.836762	0.008190	0.699905
-43.475590	-2.019354	1.841766	0.008228	0.699654
-43.890014	-1.965919	1.846771	0.008305	0.699612
-44.147664	-1.924755	1.851776	0.008353	0.699602
-43.499452	-2.035492	1.856781	0.008232	0.699612
-43.452368	-2.047098	1.861786	0.008224	0.699605
-43.887310	-1.970047	1.866790	0.008305	0.699604
-43.858230	-1.996589	1.871795	0.008300	0.699561
-44.553079	-2.016710	1.876800	0.008429	0.699268
-44.518615	-2.019262	1.881805	0.008423	0.699275
-44.982723	-1.938084	1.886810	0.008509	0.699272
-44.903890	-1.952392	1.891814	0.008495	0.699271
-44.477256	-2.024347	1.896819	0.008415	0.699279
-45.007832	-1.935004	1.901824	0.008514	0.699268
-44.636358	-2.020178	1.906829	0.008445	0.699229
-45.145146	-2.060772	1.911834	0.008540	0.698962
-45.504079	-1.997159	1.916838	0.008607	0.698961
-45.424974	-2.008634	1.921843	0.008592	0.698967
-45.263337	-2.041052	1.926848	0.008562	0.698959
-45.414270	-2.010271	1.931853	0.008590	0.698967
-45.846575	-1.936145	1.936858	0.008671	0.698960
-45.646645	-2.065146	1.941862	0.008634	0.698771
-46.209115	-2.023057	1.946867	0.008739	0.698652
-46.392743	-1.994624	1.951872	0.008773	0.698643
-46.346942	-1.999009	1.956877	0.008765	0.698651
-45.994262	-2.066381	1.961882	0.008699	0.698641
-46.292210	-2.012338	1.966886	0.008755	0.698643
-46.444451	-1.986047	1.971891	0.008783	0.698641
-46.910276	-2.044853	1.976896	0.008870	0.698352
-46.739075	-2.070186	1.981901	0.008838	0.698363
-47.326348	-1.968568	1.986906	0.008948	0.698356
-47.159054	-1.998308	1.991910	0.008917	0.698356
-46.931258	-2.036959	1.996915	0.008874	0.698360
-47.293495	-1.988175	2.001920	0.008942	0.698328

-48.019999	-2.010949	2.011917	0.009077	0.698017
-48.241914	-1.969944	2.021914	0.009119	0.698020
-48.000335	-2.012261	2.031910	0.009074	0.698021
-47.861858	-2.036418	2.041907	0.009048	0.698022
-48.276191	-1.963244	2.051904	0.009126	0.698020
-47.910170	-2.029062	2.061901	0.009058	0.698018
-48.381039	-1.945075	2.071898	0.009146	0.698018
-48.149182	-1.986272	2.081894	0.009103	0.698018
-48.209602	-1.974609	2.091891	0.009114	0.698019
-47.484411	-1.972382	2.101888	0.008979	0.698286
-47.192465	-1.990598	2.111885	0.008925	0.698355
-47.063886	-2.012298	2.121882	0.008902	0.698357
-46.939029	-2.033066	2.131878	0.008878	0.698360
-47.007006	-2.022706	2.141875	0.008891	0.698356
-47.292652	-1.970142	2.151872	0.008945	0.698359
-46.912612	-2.039497	2.161869	0.008874	0.698355
-46.940232	-1.959667	2.171866	0.008879	0.698507
-46.265635	-2.011830	2.181862	0.008754	0.698645
-46.593072	-1.952659	2.191859	0.008815	0.698646
-46.423028	-1.981407	2.201856	0.008784	0.698649
-46.283560	-1.929154	2.211853	0.008758	0.698805
-45.670528	-1.959074	2.221850	0.008644	0.698966
-45.198868	-2.042960	2.231846	0.008557	0.698966
-45.378463	-2.011542	2.241843	0.008590	0.698965
-45.318519	-1.956724	2.251840	0.008579	0.699098
-44.556532	-2.006554	2.261837	0.008437	0.699272
-44.794575	-1.962904	2.271834	0.008482	0.699274
-44.479027	-2.018870	2.281830	0.008423	0.699274
-44.159884	-1.958712	2.291827	0.008364	0.699512
-43.526859	-2.027488	2.301824	0.008247	0.699601
-43.630578	-2.007602	2.311821	0.008266	0.699603
-43.665037	-2.000954	2.321818	0.008273	0.699604
-42.910612	-2.005616	2.331814	0.008132	0.699867
-43.084194	-1.957211	2.341811	0.008165	0.699902
-42.607883	-2.041574	2.351808	0.008077	0.699903
-42.934846	-1.935924	2.361805	0.008138	0.699998
-41.779785	-2.029719	2.371802	0.007923	0.700226
-42.013618	-1.987939	2.381798	0.007966	0.700225
-42.161332	-1.961170	2.391795	0.007994	0.700226
-41.363662	-1.979587	2.401792	0.007846	0.700477
-41.266142	-1.965403	2.411789	0.007828	0.700540
-41.152153	-1.985574	2.421786	0.007807	0.700540
-40.794685	-2.004518	2.431782	0.007740	0.700631
-40.336849	-1.962872	2.441779	0.007655	0.700880
-40.178224	-1.991079	2.451776	0.007626	0.700880
-40.541298	-1.927913	2.461773	0.007694	0.700876
-39.610065	-1.990316	2.471770	0.007521	0.701086
-39.595290	-1.973695	2.481766	0.007518	0.701124
-39.377046	-2.011530	2.491763	0.007478	0.701126
-39.306719	-1.951636	2.501760	0.007465	0.701272
-38.573191	-1.999295	2.511757	0.007328	0.701440
-38.546421	-2.002445	2.521754	0.007324	0.701443
-38.584072	-1.993529	2.531750	0.007331	0.701447
-38.120907	-1.926571	2.541747	0.007245	0.701750
-37.542985	-2.029119	2.551744	0.007137	0.701750
-37.999699	-1.947716	2.561741	0.007223	0.701750
-37.158808	-1.980305	2.571738	0.007066	0.701987
-37.105405	-1.943228	2.581734	0.007057	0.702081
-36.949787	-1.971747	2.591731	0.007028	0.702079
-36.906322	-1.919908	2.601728	0.007020	0.702199
-36.172526	-1.963510	2.611725	0.006883	0.702375
-36.056119	-1.984264	2.621722	0.006862	0.702374
-36.122671	-1.963350	2.631718	0.006875	0.702392
-35.371664	-1.945063	2.641715	0.006735	0.702700
-34.951713	-2.019746	2.651712	0.006657	0.702700
-35.495829	-1.923926	2.661709	0.006758	0.702697
-34.663802	-1.975921	2.671706	0.006604	0.702891
-34.396568	-1.964681	2.681702	0.006554	0.703010
-34.344947	-1.972413	2.691699	0.006545	0.703012
-34.319450	-1.957455	2.701696	0.006540	0.703051
-33.644581	-1.931555	2.711693	0.006415	0.703346
-33.361397	-1.981617	2.721690	0.006362	0.703346
-33.576207	-1.943394	2.731686	0.006402	0.703346
-32.958390	-1.957678	2.741683	0.006288	0.703539
-32.507288	-1.989231	2.751680	0.006204	0.703637
-32.655987	-1.963221	2.761677	0.006232	0.703636
-32.382089	-1.995321	2.771674	0.006181	0.703669
-31.826495	-1.951348	2.781670	0.006078	0.703957
-31.514983	-2.007273	2.791667	0.006020	0.703956
-31.944929	-1.932632	2.801664	0.006100	0.703952
-31.154449	-1.967066	2.811661	0.005953	0.704166
-31.014557	-1.943125	2.821658	0.005927	0.704264
-30.716179	-1.996591	2.831654	0.005872	0.704263
-30.691499	-1.977032	2.841651	0.005868	0.704311
-29.920280	-1.973880	2.851648	0.005724	0.704594
-29.834924	-1.989949	2.861645	0.005709	0.704592
-29.774794	-2.000513	2.871642	0.005698	0.704592
-29.698990	-1.947193	2.881638	0.005684	0.704726
-28.788016	-2.026105	2.891635	0.005514	0.704894
-29.126054	-1.965956	2.901632	0.005577	0.704894
-29.008674	-1.988239	2.911629	0.005556	0.704890
-28.331638	-1.951168	2.921626	0.005430	0.705208
-28.060762	-1.995070	2.931622	0.005380	0.705216
-28.009556	-2.003111	2.941619	0.005370	0.705218
-28.060045	-1.928417	2.951616	0.005380	0.705350
-27.204181	-1.990469	2.961613	0.005221	0.705532
-27.271913	-1.979015	2.971610	0.005234	0.705530
-27.300715	-1.972637	2.981606	0.005239	0.705532
-26.410978	-1.968237	2.991603	0.005074	0.705860
-26.287200	-1.986182	3.001600	0.005051	0.705867
-26.237946	-1.994690	3.011597	0.005042	0.705868
-26.244323	-1.957567	3.021594	0.005043	0.705940
-25.257200	-2.036634	3.031590	0.004860	0.706134
-25.410950	-2.009303	3.041587	0.004888	0.706133
-25.775009	-1.943939	3.051584	0.004956	0.706134
-24.880781	-1.972778	3.061581	0.004790	0.706396
-24.713027	-1.977130	3.071578	0.004759	0.706447
-24.587166	-1.997932	3.081574	0.004736	0.706450
-24.399968	-1.963504	3.091571	0.004701	0.706586
-23.693970	-2.004849	3.101568	0.004570	0.706755
-23.784546	-1.988081	3.111565	0.004587	0.706756
-23.929713	-1.961931	3.121562	0.004614	0.706756
-22.971328	-1.976155	3.131558	0.004436	0.707070
-22.830603	-1.993258	3.141555	0.004410	0.707086
-23.056068	-1.952485	3.151552	0.004452	0.707087
-22.494185	-1.992956	3.161549	0.004348	0.707206
-22.219565	-1.954990	3.171546	0.004297	0.707380
-21.915672	-2.005768	3.181542	0.004241	0.707386
-22.028230	-1.987029	3.191539	0.004262	0.707383
-21.294957	-1.959144	3.201536	0.004125	0.707701
-21.309683	-1.956480	3.211533	0.004128	0.707701
-20.997577	-2.011408	3.221530	0.004070	0.707702
-20.856934	-1.956668	3.231526	0.004044	0.707862
-20.260621	-1.983984	3.241523	0.003934	0.708019
-20.361767	-1.966618	3.251520	0.003953	0.708018
-20.206357	-1.983325	3.261517	0.003924	0.708039
-19.843973	-1.890891	3.271514	0.003857	0.708354
-19.119924	-2.017249	3.281510	0.003722	0.708359
-19.225340	-1.997797	3.291507	0.003742	0.708360
-19.091400	-1.947245	3.301504	0.003717	0.708508
-18.604443	-1.964784	3.311501	0.003627	0.708647
-18.640932	-1.958086	3.321498	0.003634	0.708647
-18.411865	-1.977139	3.331494	0.003591	0.708690
-17.659299	-1.975328	3.341491	0.003451	0.708962
-17.664621	-1.974302	3.351488	0.003452	0.708961
-17.613806	-1.982109	3.361485	0.003443	0.708964
-17.506904	-1.914020	3.371482	0.003423	0.709138
-16.512122	-2.024028	3.381478	0.003238	0.709272
-16.915695	-1.950385	3.391475	0.003314	0.709275
-16.570568	-2.005098	3.401472	0.003250	0.709288
-16.104077	-1.931078	3.411469	0.003163	0.709602
-15.792326	-1.986794	3.421466	0.003105	0.709601
-15.757951	-1.993937	3.431462	0.003099	0.709599
-15.480276	-1.965150	3.441459	0.003048	0.709755
-14.978009	-1.981999	3.451456	0.002954	0.709900
-14.952971	-1.986657	3.461453	0.002950	0.709899
-15.062535	-1.967131	3.471450	0.002970	0.709899
-13.963590	-2.001727	3.481446	0.002766	0.710221
-14.162038	-1.966010	3.491443	0.002803	0.710221
-13.922881	-2.009530	3.501440	0.002759	0.710219
-14.021664	-1.942293	3.511437	0.002777	0.710318
-12.905336	-2.029656	3.521434	0.002570	0.710540
-13.124075	-1.989972	3.531430	0.002611	0.710541
-13.122658	-1.989325	3.541427	0.002611	0.710543
-12.441479	-1.997771	3.551424	0.002484	0.710768
-12.408175	-1.948240	3.561421	0.002478	0.710878
-12.200974	-1.986221	3.571418	0.002440	0.710876
-11.769666	-2.060301	3.581414	0.002360	0.710881
-11.623430	-1.965843	3.591411	0.002332	0.711121
-10.951349	-2.073114	3.601408	0.002208	0.711145
-11.165859	-2.034890	3.611405	0.002248	0.711145
-11.009867	-2.045808	3.621402	0.002219	0.711178
-10.435046	-2.005962	3.631398	0.002112	0.711462
-10.109029	-2.063862	3.641395	0.002052	0.711462
-10.180522	-2.051906	3.651392	0.002065	0.711460
-10.235881	-1.972019	3.661389	0.002076	0.711599
-9.192585	-2.074756	3.671386	0.001882	0.711765
-9.489332	-2.020037	3.681382	0.001937	0.711768
-9.410818	-2.034852	3.691379	0.001923	0.711766
-8.694609	-2.017523	3.701376	0.001789	0.712054
-8.713270	-1.996120	3.711373	0.001793	0.712090
-8.370021	-2.054813	3.721370	0.001729	0.712095
-8.440830	-1.998191	3.731366	0.001743	0.712182
-7.411717	-2.075252	3.741363	0.001551	0.712393
-7.358703	-2.083836	3.751360	0.001542	0.712395
-7.658685	-2.031720	3.761357	0.001598	0.712391
-7.117875	-2.051527	3.771354	0.001497	0.712544
-6.621628	-2.052188	3.781350	0.001405	0.712718
-6.742098	-2.029547	3.791347	0.001428	0.712720
-6.712973	-2.035993	3.801344	0.001422	0.712717
-5.933484	-2.025095	3.811341	0.001277	0.713015
-5.685877	-2.061320	3.821338	0.001232	0.713030
-5.777952	-2.043541	3.831334	0.001249	0.713032
-5.461244	-2.059362	3.841331	0.001190	0.713113
-4.827152	-2.044588	3.851328	0.001072	0.713367
-4.696806	-2.066948	3.861325	0.001048	0.713368
-4.721842	-2.062136	3.871322	0.001053	0.713368
-4.576435	-2.005325	3.881318	0.001026	0.713532
-3.704848	-2.096391	3.891315	0.000864	0.713660
-4.081085	-2.029989	3.901312	0.000934	0.713658
-3.786245	-2.081656	3.911309	0.000880	0.713659
-3.111424	-2.049218	3.921306	0.000754	0.713962
-2.996318	-2.062530	3.931302	0.000733	0.713976
-2.962048	-2.067811	3.941299	0.000727	0.713978
-3.077359	-1.989021	3.951296	0.000749	0.714093
-2.149618	-2.058440	3.961293	0.000576	0.714283
-2.122586	-2.062865	3.971290	0.000571	0.714283
-2.198762	-2.048783	3.981286	0.000586	0.714284
-1.487491	-2.030685	3.991283	0.000453	0.714571
-1.398152	-2.023340	4.001280	0.000437	0.714617
-1.571101	-1.994616	4.011277	0.000469	0.714612
-1.229043	-1.978317	4.021274	0.000406	0.714765
-1.203508	-1.907975	4.031270	0.000401	0.714914
-1.132830	-1.919111	4.041267	0.000388	0.714916
-0.759794	-1.872726	4.051264	0.000319	0.715140
-1.258428	-1.734575	4.061261	0.000412	0.715237
-0.863091	-1.751813	4.071258	0.000339	0.715342
-0.794171	-1.656661	4.081254	0.000326	0.715555
-0.724781	-1.634258	4.091251	0.000313	0.715623
-0.433527	-1.552329	4.101248	0.000259	0.715888
-0.639557	-1.489167	4.111245	0.000298	0.715940
-0.615493	-1.391891	4.121242	0.000293	0.716141
-0.864421	-1.270500	4.131238	0.000340	0.716293
-0.378819	-1.275043	4.141235	0.000249	0.716455
-0.430079	-1.130877	4.151232	0.000259	0.716722
-0.308609	-1.077061	4.161229	0.000237	0.716871
-0.259177	-0.975441	4.171226	0.000228	0.717089
-0.077728	-0.875530	4.181222	0.000194	0.717350
-0.244146	-0.749539	4.191219	0.000225	0.717541
-0.244661	-0.632909	4.201216	0.000225	0.717771
-0.453866	-0.468947	4.211213	0.000264	0.718021
-0.174641	-0.352486	4.221210	0.000212	0.718349
-0.178838	-0.230161	4.231206	0.000213	0.718588
-0.045165	-0.118017	4.241203	0.000189	0.718856
-0.063654	0.027657	4.251200	0.000192	0.719137
0.000000	0.174485	4.261197	0.000180	0.719448

0.190294	0.771002	4.266202	0.000145	0.720690
0.364628	1.991329	4.271206	0.000112	0.723149
0.567795	3.811837	4.276211	0.000073	0.726782
0.764245	6.188201	4.281216	0.000035	0.731474
0.824180	9.088154	4.286221	0.000022	0.737097
1.290735	12.396480	4.291226	-0.000067	0.743595
1.471706	16.209782	4.296230	-0.000103	0.750896
1.780943	20.402360	4.301235	-0.000164	0.758878
2.517550	24.919675	4.306240	-0.000304	0.767518
2.683122	29.907357	4.311245	-0.000338	0.776735
3.134973	35.188084	4.316250	-0.000425	0.786465
3.419021	40.824051	4.321254	-0.000481	0.796655
3.838673	46.722666	4.326259	-0.000563	0.807221
4.289525	52.916419	4.331264	-0.000651	0.818171
5.609505	59.221451	4.336269	-0.000901	0.829429
6.755714	65.809882	4.341274	-0.001119	0.840963
7.693643	72.661216	4.346278	-0.001298	0.852716
8.115772	79.802114	4.351283	-0.001381	0.864634
9.239488	87.028302	4.356288	-0.001595	0.876728
9.925204	94.489998	4.361293	-0.001727	0.888910
10.654523	102.114086	4.366298	-0.001868	0.901194
11.524050	109.867014	4.371302	-0.002035	0.913551
12.282007	117.748360	4.376307	-0.002181	0.925909
12.866883	125.796905	4.381312	-0.002295	0.938311
13.434521	133.934972	4.386317	-0.002406	0.950680
14.363983	142.100638	4.391322	-0.002584	0.963023
15.568066	150.320373	4.396326	-0.002813	0.975358
16.020110	158.735369	4.401331	-0.002903	0.987630
17.055469	167.123679	4.406336	-0.003101	0.999858
17.746337	175.588332	4.411341	-0.003235	1.011960
18.256362	184.137967	4.416346	-0.003336	1.023993
19.050171	192.677382	4.421350	-0.003489	1.035939
19.886116	201.222361	4.426355	-0.003650	1.047766
20.625001	209.837179	4.431360	-0.003793	1.059532
21.895712	218.379178	4.436365	-0.004035	1.071193
22.663509	227.023339	4.441370	-0.004184	1.082748
23.417610	235.681720	4.446374	-0.004330	1.094196
24.008324	244.356245	4.451379	-0.004445	1.105509
24.738027	253.028193	4.456384	-0.004587	1.116735
25.431555	261.661874	4.461389	-0.004721	1.127792
25.983760	270.341322	4.466394	-0.004830	1.138769
26.649738	279.006830	4.471398	-0.004959	1.149647
27.375061	287.642583	4.476403	-0.005100	1.160400
28.293227	296.227835	4.481408	-0.005276	1.171031
28.909142	304.845912	4.486413	-0.005396	1.181544
29.517080	313.475857	4.491418	-0.005515	1.191977
30.337371	322.041576	4.496422	-0.005673	1.202286
31.180872	330.598624	4.501427	-0.005836	1.212501
32.069834	339.142357	4.506432	-0.006007	1.222623
32.636293	347.741714	4.511437	-0.006118	1.232664
33.067579	356.331672	4.516442	-0.006204	1.242586
33.580497	364.886639	4.521446	-0.006305	1.252405
34.372143	373.379568	4.526451	-0.006457	1.262131
35.198342	381.881568	4.531456	-0.006617	1.271798
35.392279	390.436617	4.536461	-0.006658	1.281334
35.826765	398.958047	4.541466	-0.006745	1.290806
36.663241	407.396193	4.546470	-0.006906	1.300192
37.326279	415.892010	4.551475	-0.007035	1.309541
37.911475	424.430012	4.556480	-0.007149	1.318854
38.345910	432.851996	4.561485	-0.007235	1.327952
38.793328	441.291885	4.566490	-0.007324	1.337009
39.207176	449.700200	4.571494	-0.007407	1.345965
39.770824	458.098733	4.576499	-0.007517	1.354878
40.430590	466.457176	4.581504	-0.007645	1.363707
41.061230	474.821334	4.586509	-0.007768	1.372480
41.745599	483.168912	4.591514	-0.007901	1.381189
42.264568	491.558276	4.596518	-0.008003	1.389858
42.261162	500.002974	4.601523	-0.008007	1.398442
42.640921	508.353739	4.606528	-0.008083	1.406942
43.312554	516.662768	4.611533	-0.008214	1.415398
43.668164	525.010145	4.616538	-0.008285	1.423789
44.184865	533.337393	4.621542	-0.008387	1.432137
44.884396	541.599645	4.626547	-0.008522	1.440403
45.676484	549.876652	4.631552	-0.008675	1.448650
45.918745	558.236567	4.636557	-0.008726	1.456843
46.164664	566.573805	4.641562	-0.008777	1.464969
46.880328	574.883446	4.646566	-0.008915	1.473098
47.355577	583.154746	4.651571	-0.009009	1.481107
48.014882	591.412690	4.656576	-0.009137	1.489089
48.331366	599.719298	4.661581	-0.009201	1.497021
48.939414	607.967145	4.666586	-0.009320	1.504900
49.368942	616.264009	4.671590	-0.009405	1.512757
49.786112	624.518521	4.676595	-0.009488	1.520532
50.264717	632.782311	4.681600	-0.009583	1.528285
50.637175	641.045727	4.686605	-0.009657	1.535983
51.151785	649.270405	4.691610	-0.009758	1.543627
51.903213	657.494925	4.696614	-0.009903	1.551269
52.405855	665.729960	4.701619	-0.010002	1.558846
53.130867	673.921114	4.706624	-0.010143	1.566378
53.534617	682.181942	4.711629	-0.010223	1.573891
53.812558	690.435111	4.716634	-0.010280	1.581342
54.189267	698.687007	4.721638	-0.010355	1.588772
54.523835	706.929757	4.726643	-0.010423	1.596153
54.891637	715.151524	4.731648	-0.010497	1.603486
55.224248	723.378001	4.736653	-0.010564	1.610784
56.037815	731.536093	4.741658	-0.010721	1.618057
56.544680	739.744231	4.746662	-0.010820	1.625298
56.872698	748.009729	4.751667	-0.010887	1.632532
57.203931	756.234278	4.756672	-0.010954	1.639698
57.719765	764.387217	4.761677	-0.011055	1.646798
58.089354	772.602883	4.766682	-0.011129	1.653900
58.757638	780.747141	4.771686	-0.011259	1.660951
59.199032	788.929181	4.776691	-0.011346	1.667974
59.705064	797.134864	4.781696	-0.011445	1.674996
60.136364	805.303627	4.786701	-0.011531	1.681947
60.380282	813.519216	4.791706	-0.011582	1.688884
60.783979	821.718590	4.796710	-0.011662	1.695800
61.019644	829.905810	4.801715	-0.011711	1.702656
61.423566	838.107137	4.806720	-0.011792	1.709517
61.559357	846.330564	4.811725	-0.011822	1.716335
62.276459	854.424813	4.816730	-0.011961	1.723094
62.568923	862.605153	4.821734	-0.012021	1.729843
62.951282	870.771521	4.826739	-0.012097	1.736565
63.802636	878.868051	4.831744	-0.012261	1.743265
64.174736	887.040937	4.836749	-0.012335	1.749939
64.373707	895.252161	4.841754	-0.012377	1.756598
65.004751	903.368072	4.846758	-0.012500	1.763208
65.322645	911.535623	4.851763	-0.012565	1.769796
65.741129	919.713207	4.856768	-0.012648	1.776380
65.962805	927.880050	4.861773	-0.012694	1.782906
66.304707	936.055246	4.866778	-0.012763	1.789430
66.758729	944.249393	4.871782	-0.012853	1.795959
67.132545	952.350162	4.876787	-0.012928	1.802381
67.589379	960.496280	4.881792	-0.013018	1.808826
67.867332	968.655930	4.886797	-0.013075	1.815236
68.283206	976.777058	4.891802	-0.013158	1.821611
68.678832	984.915466	4.896806	-0.013236	1.827974
68.931557	993.083999	4.901811	-0.013289	1.834321
69.403016	1001.199389	4.906816	-0.013382	1.840631
69.659872	1009.340405	4.911821	-0.013435	1.846914
70.205825	1017.459577	4.916826	-0.013542	1.853193
70.481927	1025.618611	4.921830	-0.013598	1.859449
70.694973	1033.765275	4.926835	-0.013643	1.865667
71.248146	1041.902675	4.931840	-0.013751	1.871897
71.609148	1050.034081	4.936845	-0.013824	1.878080
71.856570	1058.161118	4.941850	-0.013875	1.884226
72.320839	1066.277579	4.946854	-0.013967	1.890368
72.850496	1074.387740	4.951859	-0.014070	1.896494
73.302697	1082.509102	4.956864	-0.014160	1.902598
73.603426	1090.647310	4.961869	-0.014221	1.908679
73.884471	1098.801229	4.966874	-0.014278	1.914750
74.195407	1106.925535	4.971878	-0.014342	1.920783
74.390752	1115.043631	4.976883	-0.014383	1.926779
74.939634	1123.164183	4.981888	-0.014491	1.932798
75.383157	1131.274251	4.986893	-0.014578	1.938779
75.816482	1139.361987	4.991898	-0.014664	1.944724
76.143902	1147.524100	4.996902	-0.014730	1.950693
76.520623	1155.652137	5.001907	-0.014806	1.956624
76.852826	1163.742606	5.006912	-0.014873	1.962505
77.256848	1171.822819	5.011917	-0.014953	1.968369
77.457602	1179.974825	5.016922	-0.014996	1.974246
77.678960	1188.100862	5.021926	-0.015042	1.980088
77.800638	1196.202892	5.026931	-0.015070	1.985885
78.374579	1204.301194	5.031936	-0.015182	1.991711
78.903680	1212.377286	5.036941	-0.015286	1.997499
78.946158	1220.506384	5.041946	-0.015299	2.003257
79.510574	1228.578713	5.046950	-0.015409	2.009012
79.917377	1236.693554	5.051955	-0.015490	2.014765
80.048290	1244.833274	5.056960	-0.015519	2.020489
80.384594	1252.921436	5.061965	-0.015587	2.026183
80.767312	1261.046190	5.066970	-0.015664	2.031891
81.027077	1269.172223	5.071974	-0.015717	2.037571
81.409347	1277.222947	5.076979	-0.015794	2.043196
81.923332	1285.306441	5.081984	-0.015894	2.048841
82.507469	1293.380628	5.086989	-0.016008	2.054471
82.736798	1301.489633	5.091994	-0.016056	2.060074
83.215754	1309.573715	5.096998	-0.016151	2.065669
83.394934	1317.706977	5.102003	-0.016189	2.071253
83.605417	1325.831675	5.107008	-0.016234	2.076819
83.773876	1333.940382	5.112013	-0.016270	2.082355
84.306897	1341.995013	5.117018	-0.016375	2.087876
84.651055	1350.118674	5.122022	-0.016444	2.093410
85.055410	1358.184327	5.127027	-0.016524	2.098896
85.431301	1366.279713	5.132032	-0.016599	2.104385
85.830415	1374.383179	5.137037	-0.016679	2.109867
86.159864	1382.536305	5.142042	-0.016745	2.115362
86.643517	1390.592061	5.147046	-0.016841	2.120792
86.887213	1398.668236	5.152051	-0.016891	2.126198
87.349724	1406.753914	5.157056	-0.016983	2.131618
87.653477	1414.843748	5.162061	-0.017044	2.137012
87.954891	1422.909944	5.167066	-0.017106	2.142376
88.447268	1430.993643	5.172070	-0.017202	2.147756
88.562422	1439.124176	5.177075	-0.017229	2.153118
89.079905	1447.177612	5.182080	-0.017331	2.158454
89.334596	1455.248535	5.187085	-0.017383	2.163764
89.565976	1463.338740	5.192090	-0.017431	2.169070
90.007378	1471.444968	5.197094	-0.017519	2.174394
90.151251	1479.532415	5.202099	-0.017551	2.179665
90.445659	1487.616516	5.207104	-0.017611	2.184935
90.773266	1495.713971	5.212109	-0.017677	2.190203
91.308291	1503.789243	5.217114	-0.017782	2.195464
91.786335	1511.841852	5.222118	-0.017876	2.200692
92.014497	1519.906403	5.227123	-0.017923	2.205893
92.168135	1528.035542	5.232128	-0.017957	2.211116
92.425930	1536.125614	5.237133	-0.018010	2.216311
93.013099	1544.151346	5.242138	-0.018125	2.221482
93.272324	1552.253771	5.247142	-0.018178	2.226661
93.627199	1560.335517	5.252147	-0.018250	2.231823
93.948509	1568.418976	5.257152	-0.018315	2.236971
94.174087	1576.495598	5.262157	-0.018362	2.242094
94.398767	1584.576368	5.267162	-0.018409	2.247208
95.023223	1592.633936	5.272166	-0.018530	2.252331
95.205041	1600.713118	5.277171	-0.018569	2.257417
95.269289	1608.831238	5.282176	-0.018586	2.262506
95.652413	1616.892439	5.287181	-0.018663	2.267575
95.945943	1625.031004	5.292186	-0.018723	2.272673
96.403330	1633.085243	5.297190	-0.018813	2.277722
97.214826	1641.050093	5.302195	-0.018969	2.282734
97.763977	1649.114643	5.307200	-0.019077	2.287775
97.959083	1657.222113	5.312205	-0.019118	2.292800
98.353122	1665.287962	5.317210	-0.019197	2.297806
98.599167	1673.381597	5.322214	-0.019248	2.302805
98.633324	1681.464779	5.327219	-0.019259	2.307769
98.872203	1689.572063	5.332224	-0.019309	2.312755
99.259435	1697.615870	5.337229	-0.019386	2.317703
99.428303	1705.678523	5.342234	-0.019423	2.322634
99.608081	1713.777492	5.347238	-0.019461	2.327577
99.783621	1721.844725	5.352243	-0.019499	2.332490
100.272663	1729.906324	5.357248	-0.019595	2.337416
100.368075	1737.982902	5.362253	-0.019618	2.342307
100.519298	1746.057218	5.367258	-0.019652	2.347192
100.949845	1754.145161	5.372262	-0.019737	2.352097
101.338625	1762.179224	5.377267	-0.019814	2.356956
101.826691	1770.201360	5.382272	-0.019910	2.361806
102.003971	1778.278565	5.387277	-0.019949	2.366654
102.380795	1786.322836	5.392282	-0.020024	2.371488
102.716743	1794.432278	5.397286	-0.020092	2.376348
102.944236	1802.470912	5.402291	-0.020139	2.381147
103.258765	1810.554802	5.407296	-0.020203	2.385971
103.286326	1818.658854	5.412301	-0.020213	2.390773
103.526645	1826.715644	5.417306	-0.020263	2.395555
103.943524	1834.756666	5.422310	-0.020346	2.400332
104.182612	1842.802119	5.427315	-0.020395	2.405088
104.473622	1850.882017	5.432320	-0.020455	2.409858
104.782349	1858.956325	5.437325	-0.020517	2.414618
105.223970	1866.986700	5.442330	-0.020605	2.419352
105.480020	1875.073734	5.447334	-0.020658	2.424096
105.774188	1883.125380	5.452339	-0.020718	2.428813
106.192720	1891.266682	5.457344	-0.020801	2.433582
106.489279	1899.303372	5.462349	-0.020861	2.438272
106.488072	1907.357476	5.467354	-0.020866	2.442940
106.964710	1915.387124	5.472358	-0.020960	2.447622
107.129887	1923.447103	5.477363	-0.020996	2.452288
107.641464	1931.477682	5.482368	-0.021096	2.456955
107.740902	1939.560429	5.487373	-0.021120	2.461611
107.855630	1947.621720	5.492378	-0.021146	2.466248
108.542076	1955.655282	5.497382	-0.021279	2.470903
108.713871	1963.735172	5.502387	-0.021316	2.475537
109.209900	1971.758026	5.507392	-0.021414	2.480154
109.549565	1979.791789	5.512397	-0.021482	2.484756
109.562231	1987.896004	5.517402	-0.021490	2.489366
110.006887	1995.974444	5.522406	-0.021578	2.493985
110.051673	2004.031628	5.527411	-0.021591	2.498554
110.497522	2012.074182	5.532416	-0.021679	2.503135
110.784171	2020.139003	5.537421	-0.021738	2.507709
111.105193	2028.214867	5.542426	-0.021803	2.512283
111.536182	2036.273748	5.547430	-0.021888	2.516848
111.721381	2044.309794	5.552435	-0.021928	2.521373
112.140820	2052.354636	5.557440	-0.022011	2.525912
112.679991	2060.382979	5.562445	-0.022117	2.530442
112.577893	2068.508543	5.567450	-0.022103	2.534972
113.058901	2076.526557	5.572454	-0.022198	2.539476
113.432241	2084.536885	5.577459	-0.022272	2.543960
113.891611	2092.600991	5.582464	-0.022363	2.548472
113.800814	2100.731227	5.587469	-0.022351	2.552973
114.176617	2108.747169	5.592474	-0.022426	2.557436
114.330345	2116.816777	5.597478	-0.022460	2.561906
114.661076	2124.841384	5.602483	-0.022527	2.566355
114.972206	2132.904450	5.607488	-0.022590	2.570816
115.216358	2140.977653	5.612493	-0.022640	2.575270
115.509585	2149.011836	5.617498	-0.022700	2.579699
115.737876	2157.073303	5.622502	-0.022748	2.584130
115.969825	2165.130010	5.627507	-0.022796	2.588552
116.306558	2173.346369	5.632512	-0.022864	2.593060
116.510654	2181.395134	5.637517	-0.022907	2.597460
116.712378	2189.378422	5.642522	-0.022950	2.601816
117.140272	2197.370907	5.647526	-0.023035	2.606186
117.201977	2205.426097	5.652531	-0.023051	2.610557
117.824616	2213.454294	5.657536	-0.023172	2.614944
118.289792	2221.456040	5.662541	-0.023264	2.619299
118.916418	2229.460659	5.667546	-0.023386	2.623659
119.093230	2237.562740	5.672550	-0.023424	2.628034
119.440338	2245.603362	5.677555	-0.023494	2.632380
119.733919	2253.667288	5.682560	-0.023554	2.636728
120.175517	2261.680134	5.687565	-0.023641	2.641051
120.441661	2269.738742	5.692570	-0.023696	2.645379
120.877644	2277.772622	5.697574	-0.023782	2.649699
121.130839	2285.844317	5.702579	-0.023834	2.654019
121.595798	2293.881711	5.707584	-0.023926	2.658328
122.242694	2301.907276	5.712589	-0.024052	2.662636
122.340429	2309.993736	5.717594	-0.024075	2.666933
122.523754	2318.095273	5.722598	-0.024114	2.671237
122.740583	2326.168114	5.727603	-0.024160	2.675520
123.179535	2334.188030	5.732608	-0.024247	2.679783
123.173889	2342.241641	5.737613	-0.024251	2.684029
123.472325	2350.262336	5.742618	-0.024311	2.688270
123.872522	2358.325803	5.747622	-0.024391	2.692533
123.858960	2366.395592	5.752627	-0.024394	2.696767
124.209983	2374.425245	5.757632	-0.024464	2.700995
124.573836	2382.434492	5.762637	-0.024537	2.705207
124.652081	2390.505654	5.767642	-0.024557	2.709427
125.018265	2398.582537	5.772646	-0.024630	2.713662
125.156268	2406.608913	5.777651	-0.024661	2.717849
125.367909	2414.640768	5.782656	-0.024706	2.722037
125.536576	2422.701079	5.787661	-0.024742	2.726231
125.694568	2430.746236	5.792666	-0.024777	2.730410
126.064726	2438.795525	5.797670	-0.024851	2.734597
126.586901	2446.795803	5.802675	-0.024953	2.738762
126.749443	2454.839630	5.807680	-0.024989	2.742922
126.997702	2462.892310	5.812685	-0.025040	2.747084
127.227516	2470.986261	5.817690	-0.025088	2.751260
127.831622	2479.088722	5.822694	-0.025206	2.755457
128.185150	2487.057847	5.827699	-0.025276	2.759564
128.346114	2495.092175	5.832704	-0.025312	2.763687
128.469402	2503.142402	5.837709	-0.025340	2.767809
128.484232	2511.218012	5.842714	-0.025348	2.771932
128.763391	2519.266812	5.847718	-0.025405	2.776050
128.897145	2527.279608	5.852723	-0.025435	2.780136
129.047278	2535.306055	5.857728	-0.025468	2.784223
129.385315	2543.359494	5.862733	-0.025536	2.788329
129.512674	2551.417998	5.867738	-0.025565	2.792419
129.774644	2559.475273	5.872742	-0.025619	2.796511
129.855939	2567.494888	5.877747	-0.025639	2.800567
130.257465	2575.489209	5.882752	-0.025719	2.804622
130.504296	2583.545419	5.887757	-0.025770	2.808694
130.795753	2591.606467	5.892762	-0.025829	2.812765
131.380113	2599.646964	5.897766	-0.025943	2.816837
131.375111	2607.677299	5.902771	-0.025947	2.820864
131.814670	2615.703782	5.907776	-0.026034	2.824908
132.097535	2623.768050	5.912781	-0.026092	2.828957
132.251552	2631.837461	5.917786	-0.026126	2.832995
132.358086	2639.913860	5.922790	-0.026151	2.837028
132.749204	2647.884126	5.927795	-0.026229	2.841019
133.097242	2655.890816	5.932800	-0.026299	2.845019
133.265727	2663.965816	5.937805	-0.026335	2.849038
133.576364	2672.007252	5.942810	-0.026398	2.853042
133.857565	2680.067905	5.947814	-0.026456	2.857049
133.919279	2688.112958	5.952819	-0.026473	2.861029
134.221391	2696.138409	5.957824	-0.026534	2.865008
134.336167	2704.213976	5.962829	-0.026561	2.868996
134.639215	2712.241663	5.967834	-0.026622	2.872965
134.897206	2720.294564	5.972838	-0.026675	2.876939
134.959960	2728.334111	5.977843	-0.026692	2.880889
135.473861	2736.336958	5.982848	-0.026793	2.884841
135.829842	2744.364821	5.987853	-0.026864	2.888791
135.943191	2752.436595	5.992858	-0.026891	2.892744
136.199508	2760.495935	5.997862	-0.026943	2.896693
136.458328	2768.517449	6.002867	-0.026997	2.900618
136.767856	2776.527687	6.007872	-0.027059	2.904535
136.970514	2784.592189	6.012877	-0.027102	2.908468
137.152297	2792.696400	6.017882	-0.027141	2.912413
137.297073	2800.790007	6.022886	-0.027174	2.916346
137.521685	2808.749752	6.027891	-0.027220	2.920213
137.933763	2816.723526	6.032896	-0.027302	2.924091
138.322082	2824.744993	6.037901	-0.027380	2.927986
138.160452	2832.854255	6.042906	-0.027355	2.931889
138.637983	2840.870196	6.047910	-0.027449	2.935776
138.783389	2848.881213	6.052915	-0.027481	2.939637
139.078293	2856.896362	6.057920	-0.027541	2.943504
139.344616	2864.948753	6.062925	-0.027596	2.947381
139.601761	2873.003762	6.067930	-0.027649	2.951254
139.704333	2881.085545	6.072934	-0.027673	2.955127
139.608778	2889.089543	6.077939	-0.027660	2.958948
140.164638	2897.095240	6.082944	-0.027769	2.962797
140.387272	2905.144837	6.087949	-0.027816	2.966646
140.353695	2913.206901	6.092954	-0.027815	2.970482
140.798538	2921.254437	6.097958	-0.027902	2.974331
140.990418	2929.262038	6.102963	-0.027943	2.978143
141.160994	2937.293479	6.107968	-0.027980	2.981960
141.397227	2945.338870	6.112973	-0.028029	2.985782
141.588457	2953.375049	6.117978	-0.028070	2.989593
141.968108	2961.466408	6.122982	-0.028146	2.993435
142.171786	2969.449272	6.127987	-0.028189	2.997211
142.659987	2977.455339	6.132992	-0.028285	3.001008
142.761905	2985.484680	6.137997	-0.028309	3.004791
142.905969	2993.527074	6.143002	-0.028341	3.008578
143.352220	3001.583859	6.148006	-0.028429	3.012382
143.410193	3009.638496	6.153011	-0.028445	3.016161
143.709821	3017.643937	6.158016	-0.028506	3.019924
143.792365	3025.688230	6.163021	-0.028527	3.023690
143.994217	3033.706073	6.168026	-0.028569	3.027444
144.376266	3041.778839	6.173030	-0.028646	3.031228
144.501630	3049.830912	6.178035	-0.028674	3.034986
144.643084	3057.844369	6.183040	-0.028706	3.038721
144.920908	3065.874484	6.188045	-0.028762	3.042466
145.058133	3073.902255	6.193050	-0.028793	3.046199
145.319360	3081.954786	6.198054	-0.028847	3.049944
145.583534	3090.003560	6.203059	-0.028901	3.053684
145.897018	3098.024850	6.208064	-0.028965	3.057408
145.799832	3106.105655	6.213069	-0.028952	3.061135
145.957829	3114.082107	6.218074	-0.028986	3.064823
146.266779	3122.145033	6.223078	-0.029049	3.068552
146.579018	3130.204023	6.228083	-0.029112	3.072275
146.806763	3138.282918	6.233088	-0.029160	3.075999
147.264708	3146.239462	6.238093	-0.029250	3.079673
147.163918	3154.279440	6.243098	-0.029237	3.083355
147.384074	3162.314916	6.248102	-0.029283	3.087045
147.541462	3170.326858	6.253107	-0.029317	3.090717
147.627823	3178.388395	6.258112	-0.029338	3.094404
147.624661	3186.443279	6.263117	-0.029343	3.098080
148.025663	3194.411626	6.268122	-0.029423	3.101730
148.261644	3202.465123	6.273126	-0.029472	3.105407
148.529847	3210.489345	6.278131	-0.029527	3.109068
148.910591	3218.545633	6.283136	-0.029603	3.112744
149.130602	3226.584969	6.288141	-0.029649	3.116401
149.174028	3234.581796	6.293146	-0.029662	3.120026
149.450748	3242.616562	6.298150	-0.029719	3.123675
149.590169	3250.634391	6.303155	-0.029750	3.127306
149.780673	3258.683546	6.308160	-0.029791	3.130948
149.950128	3266.765728	6.313165	-0.029827	3.134601
150.221430	3274.739216	6.318170	-0.029883	3.138205
150.681737	3282.777027	6.323174	-0.029974	3.141841
150.826803	3290.791367	6.328179	-0.030006	3.145450
151.005131	3298.842352	6.333184	-0.030044	3.149071
151.278623	3306.919879	6.338189	-0.030100	3.152705
151.288009	3314.956595	6.343194	-0.030107	3.156305
151.550462	3322.961808	6.348198	-0.030161	3.159897
151.894067	3330.951609	6.353203	-0.030230	3.163482
151.895601	3339.004805	6.358208	-0.030236	3.167077
152.069022	3347.065244	6.363213	-0.030273	3.170677
152.347330	3355.069397	6.368218	-0.030330	3.174254
152.873363	3363.105206	6.373222	-0.030433	3.177851
153.067359	3371.129583	6.378227	-0.030474	3.181424
153.151079	3379.159589	6.383232	-0.030495	3.184991
153.533145	3387.186283	6.388237	-0.030571	3.188566
153.730282	3395.229977	6.393242	-0.030613	3.192136
154.097474	3403.303289	6.398246	-0.030687	3.195722
154.216048	3411.300635	6.403251	-0.030714	3.199260
154.385787	3419.335308	6.408256	-0.030751	3.202813
154.479421	3427.358570	6.413261	-0.030773	3.206354
154.794110	3435.361331	6.418266	-0.030837	3.209890
154.869272	3443.452507	6.423270	-0.030856	3.213452
155.008929	3451.485484	6.428275	-0.030887	3.216987
155.057003	3459.508935	6.433280	-0.030901	3.220511
155.409202	3467.498420	6.438285	-0.030972	3.224028
155.542879	3475.529394	6.443290	-0.031002	3.227550
155.969721	3483.577530	6.448294	-0.031087	3.231088
156.346160	3491.658707	6.453299	-0.031162	3.234634
156.479305	3499.643469	6.458304	-0.031192	3.238124
156.641885	3507.676457	6.463309	-0.031227	3.241633
156.850007	3515.654485	6.468314	-0.031271	3.245116
157.292650	3523.694185	6.473318	-0.031359	3.248631
157.497398	3531.745356	6.478323	-0.031402	3.252138
157.723775	3539.803333	6.483328	-0.031449	3.255645
157.901544	3547.808309	6.488333	-0.031487	3.259124
158.281816	3555.789664	6.493338	-0.031563	3.262596
158.621267	3563.836148	6.498342	-0.031632	3.266091
158.587627	3571.897293	6.503347	-0.031631	3.269574
158.888555	3579.943062	6.508352	-0.031692	3.273060
159.439851	3587.965392	6.513357	-0.031800	3.276541
159.496229	3595.959488	6.518362	-0.031815	3.279988
159.942378	3603.989169	6.523366	-0.031903	3.283461
159.957811	3612.034502	6.528371	-0.031911	3.286920
160.113820	3620.088751	6.533376	-0.031946	3.290385
160.465442	3628.145634	6.538381	-0.032016	3.293855
160.435555	3636.130259	6.543386	-0.032016	3.297276
160.615140	3644.192698	6.548390	-0.032054	3.300735
160.902930	3652.170758	6.553395	-0.032113	3.304158
161.181189	3660.218771	6.558400	-0.032170	3.307607
161.362565	3668.293457	6.563405	-0.032209	3.311060
161.551590	3676.326898	6.568410	-0.032249	3.314492
161.723879	3684.359243	6.573414	-0.032286	3.317919
162.151800	3692.323801	6.578419	-0.032371	3.321323
162.185950	3700.332192	6.583424	-0.032383	3.324728
162.342057	3708.373401	6.588429	-0.032417	3.328148
162.540605	3716.395671	6.593434	-0.032459	3.331558
163.057532	3724.435980	6.598438	-0.032560	3.334984
162.846805	3732.470902	6.603443	-0.032526	3.338377
163.214021	3740.477553	6.608448	-0.032600	3.341776
163.549823	3748.496010	6.613453	-0.032667	3.345175
163.570923	3756.535300	6.618458	-0.032676	3.348568
163.832914	3764.631555	6.623462	-0.032730	3.351990
164.138672	3772.674577	6.628467	-0.032792	3.355388
164.181243	3780.657263	6.633472	-0.032806	3.358748
164.485090	3788.677523	6.638477	-0.032867	3.362129
164.579787	3796.681549	6.643482	-0.032890	3.365493
164.787127	3804.740591	6.648486	-0.032934	3.368880
164.702931	3812.785043	6.653491	-0.032923	3.372248
165.094368	3820.825320	6.658496	-0.033001	3.375627
165.351589	3828.832221	6.663501	-0.033054	3.378984
165.336904	3836.867293	6.668506	-0.033057	3.382340
165.731900	3844.897371	6.673510	-0.033135	3.385705
165.959232	3852.910831	6.678515	-0.033183	3.389053
166.044071	3861.006588	6.683520	-0.033204	3.392428
166.369114	3869.071492	6.688525	-0.033269	3.395795
166.631337	3876.977734	6.693530	-0.033323	3.399090
166.789022	3885.024644	6.698534	-0.033358	3.402437
166.860189	3893.037085	6.703539	-0.033376	3.405763
167.115369	3901.024736	6.708544	-0.033429	3.409082
167.365705	3909.078794	6.713549	-0.033481	3.412425
167.559721	3917.127419	6.718554	-0.033522	3.415761
168.006339	3925.105667	6.723558	-0.033610	3.419072
168.248710	3933.133689	6.728563	-0.033660	3.422395
168.404823	3941.176732	6.733568	-0.033695	3.425717
168.662641	3949.204148	6.738573	-0.033748	3.429033
168.914176	3957.271092	6.743578	-0.033800	3.432361
168.988964	3965.330811	6.748582	-0.033819	3.435678
169.061132	3973.311890	6.753587	-0.033837	3.438959
169.371175	3981.317054	6.758592	-0.033900	3.442254
169.596795	3989.340702	6.763597	-0.033947	3.445551
169.619884	3997.361851	6.768602	-0.033957	3.448838
169.713805	4005.452883	6.773606	-0.033979	3.452152
169.920868	4013.497547	6.778611	-0.034023	3.455447
170.159802	4021.470957	6.783616	-0.034073	3.458712
170.230950	4029.556562	6.788621	-0.034091	3.462013
170.446960	4037.518809	6.793626	-0.034136	3.465266
170.640951	4045.589337	6.798630	-0.034178	3.468559
170.769369	4053.622184	6.803635	-0.034207	3.471832
171.078134	4061.652201	6.808640	-0.034269	3.475106
171.400690	4069.648853	6.813645	-0.034334	3.478363
171.465694	4077.651949	6.818650	-0.034352	3.481612
171.680207	4085.675434	6.823654	-0.034397	3.484871
171.793103	4093.670560	6.828659	-0.034423	3.488113
171.908468	4101.750190	6.833664	-0.034449	3.491385
171.979169	4109.798454	6.838669	-0.034468	3.494641
172.325594	4117.768548	6.843674	-0.034537	3.497870
172.430258	4125.817637	6.848678	-0.034562	3.501121
172.554204	4133.792173	6.853683	-0.034590	3.504339
173.039901	4141.825201	6.858688	-0.034686	3.507589
173.225906	4149.917012	6.863693	-0.034726	3.510850
173.148725	4157.914718	6.868698	-0.034716	3.514062
173.222497	4165.968778	6.873702	-0.034735	3.517299
173.792787	4173.927613	6.878707	-0.034846	3.520509
173.847004	4181.910071	6.883712	-0.034862	3.523711
173.943775	4189.998747	6.888717	-0.034885	3.526953
174.017686	4198.020931	6.893722	-0.034904	3.530165
174.469377	4206.057737	6.898726	-0.034993	3.533391
174.434742	4214.115451	6.903731	-0.034992	3.536608
174.820344	4222.086140	6.908736	-0.035069	3.539800
175.243538	4230.120924	6.913741	-0.035153	3.543016
175.259998	4238.153761	6.918746	-0.035161	3.546215
175.595264	4246.175479	6.923750	-0.035228	3.549417
175.762727	4254.291778	6.928755	-0.035265	3.552649
175.870455	4262.345295	6.933760	-0.035290	3.555851
176.086199	4270.312306	6.938765	-0.035335	3.559019
176.338651	4278.282223	6.943770	-0.035387	3.562186
176.519168	4286.291482	6.948774	-0.035426	3.565364
176.738311	4294.328015	6.953779	-0.035472	3.568551
176.916142	4302.378826	6.958784	-0.035510	3.571739
177.196062	4310.419943	6.963789	-0.035567	3.574924
177.139267	4318.409118	6.968794	-0.035562	3.578076
177.416107	4326.450672	6.973798	-0.035619	3.581255
177.799343	4334.427550	6.978803	-0.035695	3.584409
178.056416	4342.454114	6.983808	-0.035748	3.587576
177.967175	4350.532816	6.988813	-0.035737	3.590750
178.277867	4358.528559	6.993818	-0.035800	3.593901
178.422348	4366.579233	6.998822	-0.035832	3.597066
178.621968	4374.568613	7.003827	-0.035874	3.600205
178.752625	4382.549281	7.008832	-0.035903	3.603337
178.831730	4390.606843	7.013837	-0.035923	3.606494
178.981387	4398.619380	7.018842	-0.035956	3.609633
179.168762	4406.675442	7.023846	-0.035996	3.612787
179.254378	4414.713852	7.028851	-0.036017	3.615929
179.348993	4422.711437	7.033856	-0.036040	3.619052
179.680972	4430.725697	7.038861	-0.036107	3.622186
179.678645	4438.744076	7.043866	-0.036112	3.625309
180.174827	4446.779398	7.048870	-0.036209	3.628450
180.413264	4454.831081	7.053875	-0.036259	3.631587
180.480544	4462.880057	7.058880	-0.036276	3.634716
180.867227	4470.882438	7.063885	-0.036353	3.637832
180.774275	4478.902537	7.068890	-0.036341	3.640940
180.885086	4486.898452	7.073894	-0.036367	3.644042
181.093479	4494.930009	7.078899	-0.036411	3.647157
181.279786	4502.946635	7.083904	-0.036451	3.650263
181.288957	4511.025949	7.088909	-0.036458	3.653386
181.402400	4519.037128	7.093914	-0.036484	3.656483
181.706731	4527.027585	7.098918	-0.036546	3.659574
181.771450	4535.048504	7.103923	-0.036563	3.662668
181.854214	4543.100966	7.108928	-0.036583	3.665772
182.308924	4551.128691	7.113933	-0.036673	3.668873
182.491538	4559.163868	7.118938	-0.036712	3.671968
182.769613	4567.178368	7.123942	-0.036769	3.675054
182.851878	4575.201451	7.128947	-0.036790	3.678136
183.195993	4583.183703	7.133952	-0.036859	3.681206
183.354617	4591.198162	7.138957	-0.036894	3.684282
183.186705	4599.238614	7.143962	-0.036867	3.687356
183.526691	4607.266803	7.148966	-0.036936	3.690437
183.713854	4615.323376	7.153971	-0.036976	3.693521
183.748163	4623.331409	7.158976	-0.036987	3.696581
184.054067	4631.336473	7.163981	-0.037049	3.699643
184.057220	4639.338620	7.168986	-0.037055	3.702695
184.041130	4647.382240	7.173990	-0.037057	3.705759
184.319596	4655.408452	7.178995	-0.037114	3.708822
184.658070	4663.453142	7.184000	-0.037182	3.711890
184.909831	4671.552981	7.189005	-0.037234	3.714974
184.924607	4679.512903	7.194010	-0.037242	3.717997
185.365928	4687.518604	7.199014	-0.037330	3.721046
185.559688	4695.471949	7.204019	-0.037371	3.724066
185.616386	4703.486762	7.209024	-0.037386	3.727103
185.889912	4711.520755	7.214029	-0.037442	3.730150
185.928743	4719.580462	7.219034	-0.037455	3.733199
186.165338	4727.611960	7.224038	-0.037504	3.736240
186.292031	4735.587553	7.229043	-0.037533	3.739254
186.400466	4743.648613	7.234048	-0.037558	3.742298
186.542444	4751.669446	7.239053	-0.037590	3.745325
186.603376	4759.672046	7.244058	-0.037606	3.748340
187.042236	4767.759672	7.249062	-0.037693	3.751394
187.322945	4775.740148	7.254067	-0.037750	3.754401
187.452178	4783.749824	7.259072	-0.037780	3.757414
187.836859	4791.800153	7.264077	-0.037856	3.760445
188.146749	4799.759340	7.269082	-0.037919	3.763438
188.379543	4807.813891	7.274086	-0.037968	3.766462
188.454309	4815.853823	7.279091	-0.037987	3.769475
188.894137	4823.877996	7.284096	-0.038074	3.772488
188.890603	4831.938202	7.289101	-0.038078	3.775501
189.009647	4839.932231	7.294106	-0.038105	3.778491
189.289338	4847.956426	7.299110	-0.038163	3.781492
189.508726	4855.953072	7.304115	-0.038209	3.784480
189.443358	4864.007561	7.309120	-0.038202	3.787481
189.712713	4872.054293	7.314125	-0.038257	3.790483
189.730779	4880.077169	7.319130	-0.038265	3.793469
190.069956	4888.108325	7.324134	-0.038334	3.796463
190.132978	4896.063954	7.329139	-0.038350	3.799420
190.344610	4904.068373	7.334144	-0.038395	3.802396
190.540175	4912.119678	7.339149	-0.038437	3.805387
190.613711	4920.095238	7.344154	-0.038455	3.808345
190.900217	4928.152307	7.349158	-0.038514	3.811335
191.049755	4936.142785	7.354163	-0.038547	3.814296
191.112976	4944.187621	7.359168	-0.038564	3.817272
191.543028	4952.216729	7.364173	-0.038649	3.820248
191.718253	4960.237358	7.369178	-0.038687	3.823213
191.667820	4968.268782	7.374182	-0.038682	3.826174
191.895607	4976.287111	7.379187	-0.038730	3.829135
192.050638	4984.283678	7.384192	-0.038764	3.832084
192.408144	4992.343710	7.389197	-0.038836	3.835058
192.273525	5000.318282	7.394202	-0.038816	3.837988
192.376805	5008.355163	7.399206	-0.038840	3.840943
192.883070	5016.350111	7.404211	-0.038939	3.843890
192.941238	5024.360354	7.409216	-0.038955	3.846830
192.980999	5032.453600	7.414221	-0.038968	3.849798
193.063224	5040.457831	7.419226	-0.038988	3.852732
193.409676	5048.509863	7.424230	-0.039058	3.855687
193.665848	5056.513449	7.429235	-0.039111	3.858620
193.494880	5064.517707	7.434240	-0.039084	3.861542
193.904373	5072.522623	7.439245	-0.039165	3.864474
193.981757	5080.555382	7.444250	-0.039185	3.867407
194.364679	5088.606753	7.449254	-0.039261	3.870350
194.614740	5096.818204	7.454259	-0.039313	3.873348
194.848869	5104.843137	7.459264	-0.039362	3.876274
194.875627	5112.748072	7.464269	-0.039372	3.879151
194.865626	5120.751066	7.469274	-0.039375	3.882060
195.181446	5128.715125	7.474278	-0.039439	3.884960
195.221636	5136.723197	7.479283	-0.039452	3.887867
195.266761	5144.750802	7.484288	-0.039465	3.890780
195.570634	5152.797468	7.489293	-0.039527	3.893703
195.353374	5160.820019	7.494298	-0.039492	3.896604
195.604876	5168.803130	7.499302	-0.039544	3.899498
196.005241	5176.833719	7.504307	-0.039623	3.902410
196.287625	5184.825648	7.509312	-0.039681	3.905304
196.410102	5192.871721	7.514317	-0.039709	3.908212
196.232726	5200.903012	7.519322	-0.039681	3.911106
196.543434	5208.931478	7.524326	-0.039744	3.914007
196.658583	5216.960480	7.529331	-0.039771	3.916902
196.663883	5224.914356	7.534336	-0.039777	3.919766
197.066922	5232.940591	7.539341	-0.039857	3.922661
197.027604	5240.973679	7.544346	-0.039855	3.925548
197.196987	5248.994289	7.549350	-0.039891	3.928433
197.490507	5257.008529	7.554355	-0.039951	3.931315
197.542755	5265.003454	7.559360	-0.039966	3.934184
197.757540	5273.079762	7.564365	-0.040011	3.937082
197.706467	5281.073344	7.569370	-0.040007	3.939945
198.103117	5289.057493	7.574374	-0.040086	3.942809
198.164043	5297.084299	7.579379	-0.040102	3.945681
198.115243	5305.105783	7.584384	-0.040098	3.948547
198.597273	5313.164773	7.589389	-0.040193	3.951434
198.626850	5321.207331	7.594394	-0.040204	3.954305
198.853153	5329.189259	7.599398	-0.040251	3.957155
198.911434	5337.219364	7.604403	-0.040267	3.960018
199.189646	5345.179798	7.609408	-0.040324	3.962857
199.457635	5353.205362	7.614413	-0.040379	3.965717
199.526394	5361.220905	7.619418	-0.040397	3.968569
199.754828	5369.290012	7.624422	-0.040444	3.971440
199.841587	5377.342761	7.629427	-0.040466	3.974300
199.962832	5385.347792	7.634432	-0.040493	3.977143
200.409019	5393.344190	7.639437	-0.040582	3.979985
200.454673	5401.352057	7.644442	-0.040595	3.982823
200.554789	5409.368411	7.649446	-0.040619	3.985663
200.690493	5417.400353	7.654451	-0.040649	3.988507
200.995428	5425.442624	7.659456	-0.040711	3.991355
201.107708	5433.494355	7.664461	-0.040737	3.994201
201.184305	5441.534943	7.669466	-0.040757	3.997041
201.292406	5449.511681	7.674470	-0.040782	3.999857
201.455076	5457.541219	7.679475	-0.040817	4.002690
201.621752	5465.508076	7.684480	-0.040854	4.005499
201.956262	5473.547550	7.689485	-0.040921	4.008335
202.060134	5481.602343	7.694490	-0.040945	4.011170
202.185453	5489.645045	7.699494	-0.040974	4.013999
202.427506	5497.674055	7.704499	-0.041024	4.016823
202.605102	5505.623603	7.709504	-0.041062	4.019616
202.796918	5513.683192	7.714509	-0.041103	4.022446
202.809733	5521.671775	7.719514	-0.041111	4.025247
203.173212	5529.705861	7.724518	-0.041183	4.028067
203.381430	5537.749827	7.729523	-0.041227	4.030885
203.314863	5545.858759	7.734528	-0.041220	4.033721
203.666548	5553.871327	7.739533	-0.041291	4.036527
203.668683	5561.771433	7.744538	-0.041296	4.039286
204.020549	5569.833765	7.749542	-0.041367	4.042106
204.141225	5577.788172	7.754547	-0.041394	4.044882
204.275372	5585.812040	7.759552	-0.041424	4.047681
204.387683	5593.839758	7.764557	-0.041451	4.050479
204.643674	5601.872425	7.769562	-0.041503	4.053279
204.775116	5609.913277	7.774566	-0.041533	4.056078
204.901396	5617.909647	7.779571	-0.041562	4.058859
205.188652	5625.928266	7.784576	-0.041620	4.061649
205.414000	5633.920890	7.789581	-0.041667	4.064426
205.653780	5641.918490	7.794586	-0.041717	4.067204
205.793898	5649.987901	7.799590	-0.041748	4.070003
205.973335	5658.028877	7.804595	-0.041787	4.072791
205.900035	5665.991845	7.809600	-0.041778	4.075547
206.214795	5674.026706	7.814605	-0.041842	4.078331
206.080538	5682.043631	7.819610	-0.041822	4.081100
206.420844	5690.051549	7.824614	-0.041891	4.083871
206.859958	5698.089178	7.829619	-0.041977	4.086652
206.787560	5706.071195	7.834624	-0.041969	4.089405
207.115571	5714.129799	7.839629	-0.042035	4.092187
207.048927	5722.159605	7.844634	-0.042028	4.094953
207.228390	5730.167101	7.849638	-0.042067	4.097712
207.351080	5738.189536	7.854643	-0.042095	4.100474
207.593751	5746.158314	7.859648	-0.042145	4.103217
207.749986	5754.241285	7.864653	-0.042179	4.105996
207.730071	5762.240105	7.869658	-0.042180	4.108742
207.988701	5770.274667	7.874662	-0.042234	4.111502
208.099221	5778.357677	7.879667	-0.042260	4.114275
208.109864	5786.330544	7.884672	-0.042267	4.117007
208.368598	5794.339583	7.889677	-0.042320	4.119753
208.512129	5802.324591	7.894682	-0.042352	4.122487
208.617050	5810.315481	7.899686	-0.042376	4.125221
208.719027	5818.380370	7.904691	-0.042401	4.127978
208.978314	5826.380935	7.909696	-0.042454	4.130714
209.301633	5834.444069	7.914701	-0.042519	4.133470
209.300637	5842.471349	7.919706	-0.042524	4.136207
209.382759	5850.423075	7.924710	-0.042545	4.138919
209.549384	5858.550330	7.929715	-0.042581	4.141689
209.746850	5866.466382	7.934720	-0.042623	4.144386
210.016595	5874.529268	7.939725	-0.042678	4.147131
210.034988	5882.555934	7.944730	-0.042687	4.149860
210.329187	5890.623291	7.949734	-0.042746	4.152604
210.503861	5898.599076	7.954739	-0.042784	4.155313
210.529139	5906.582556	7.959744	-0.042794	4.158022
210.932151	5914.661428	7.964749	-0.042874	4.160766
210.956159	5922.633416	7.969754	-0.042884	4.163467
211.087324	5930.652147	7.974758	-0.042913	4.166183
211.272911	5938.668793	7.979763	-0.042953	4.168898
211.298521	5946.714604	7.984768	-0.042963	4.171619
211.720093	5954.730257	7.989773	-0.043046	4.174332
211.902182	5962.765745	7.994778	-0.043085	4.177048
211.851477	5970.729102	7.999782	-0.043081	4.179734
211.996594	5978.762436	8.004787	-0.043113	4.182445
212.313642	5986.753731	8.009792	-0.043177	4.185142
212.761967	5994.805398	8.014797	-0.043266	4.187859
212.627358	6002.807078	8.019802	-0.043246	4.190551
212.691541	6010.951385	8.024806	-0.043263	4.193291
213.037840	6018.983355	8.029811	-0.043333	4.195994
213.055574	6026.880466	8.034816	-0.043341	4.198648
213.100997	6034.912879	8.039821	-0.043355	4.201345
213.332989	6042.856206	8.044826	-0.043403	4.204012
213.458090	6050.901150	8.049830	-0.043431	4.206711
213.535859	6058.913636	8.054835	-0.043451	4.209396
213.592551	6066.952444	8.059840	-0.043467	4.212089
213.942203	6074.992147	8.064845	-0.043537	4.214783
214.029973	6082.991860	8.069850	-0.043558	4.217459
214.237106	6090.982820	8.074854	-0.043602	4.220132
214.340328	6099.010101	8.079859	-0.043627	4.222814
214.323203	6106.989979	8.084864	-0.043628	4.225477
214.451008	6115.059548	8.089869	-0.043657	4.228170
214.739286	6123.063093	8.094874	-0.043716	4.230841
214.963592	6131.076499	8.099878	-0.043763	4.233513
215.025434	6139.129792	8.104883	-0.043780	4.236195
215.145481	6147.106762	8.109888	-0.043807	4.238850
215.376031	6155.136347	8.114893	-0.043855	4.241522
215.444486	6163.092998	8.119898	-0.043873	4.244167
215.579750	6171.145861	8.124902	-0.043903	4.246842
215.647936	6179.194451	8.129907	-0.043921	4.249514
215.735767	6187.221232	8.134912	-0.043943	4.252177
216.110707	6195.247983	8.139917	-0.044018	4.254841
216.132750	6203.238694	8.144922	-0.044027	4.257488
216.458012	6211.281795	8.149926	-0.044093	4.260154
216.596073	6219.291713	8.154931	-0.044123	4.262805
216.735155	6227.286817	8.159936	-0.044154	4.265450
216.939387	6235.365548	8.164941	-0.044198	4.268121
217.029080	6243.399499	8.169946	-0.044219	4.270775
217.213672	6251.416126	8.174950	-0.044259	4.273422
217.384069	6259.506354	8.179955	-0.044296	4.276091
217.300500	6267.386565	8.184960	-0.044285	4.278688
217.684531	6275.480438	8.189965	-0.044362	4.281357
217.933288	6283.413155	8.194970	-0.044413	4.283971
217.975278	6291.490849	8.199974	-0.044426	4.286628
218.075779	6299.445779	8.204979	-0.044450	4.289245
218.064807	6307.497732	8.209984	-0.044453	4.291890
218.473829	6315.562353	8.214989	-0.044535	4.294542
218.587774	6323.553714	8.219994	-0.044561	4.297165
218.681339	6331.574312	8.224998	-0.044583	4.299796
218.889343	6339.600920	8.230003	-0.044627	4.302429
219.046196	6347.578462	8.235008	-0.044662	4.305043
219.173257	6355.632225	8.240013	-0.044690	4.307681
219.503225	6363.610798	8.245018	-0.044757	4.310293
219.273685	6371.699103	8.250022	-0.044719	4.312936
219.564265	6379.696142	8.255027	-0.044779	4.315552
219.805460	6387.648605	8.260032	-0.044829	4.318150
220.190419	6395.694555	8.265037	-0.044905	4.320779
220.266856	6403.675927	8.270042	-0.044925	4.323383
220.610108	6411.683965	8.275046	-0.044994	4.325996
220.919675	6419.750465	8.280051	-0.045057	4.328626
220.887267	6427.751816	8.285056	-0.045056	4.331230
221.243678	6435.817660	8.290061	-0.045127	4.333857
221.508067	6443.812740	8.295066	-0.045181	4.336459
221.603161	6451.785603	8.300070	-0.045204	4.339050
221.776084	6459.842402	8.305075	-0.045242	4.341668
221.671383	6467.772381	8.310080	-0.045227	4.344241
221.986575	6475.840775	8.315085	-0.045291	4.346861
222.174250	6483.882119	8.320090	-0.045331	4.349469
222.122438	6491.940973	8.325094	-0.045327	4.352079
222.475490	6499.993573	8.330099	-0.045397	4.354689
222.591217	6507.984490	8.335104	-0.045424	4.357276
222.844588	6515.938852	8.340109	-0.045476	4.359850
222.855514	6523.939502	8.345114	-0.045484	4.362436
223.005398	6531.924806	8.350118	-0.045517	4.365016
223.273683	6540.019035	8.355123	-0.045572	4.367631
223.246645	6547.975759	8.360128	-0.045572	4.370198
223.639925	6556.009618	8.365133	-0.045650	4.372790
223.726399	6564.064797	8.370138	-0.045671	4.375387
223.766668	6572.013172	8.375142	-0.045684	4.377947
224.199254	6580.044436	8.380147	-0.045770	4.380534
224.207910	6588.034897	8.385152	-0.045776	4.383105
224.396182	6596.092903	8.390157	-0.045817	4.385696
224.388673	6604.091182	8.395162	-0.045820	4.388266
224.486791	6612.128290	8.400166	-0.045844	4.390847
224.667460	6620.172639	8.405171	-0.045882	4.393430
224.806552	6628.209854	8.410176	-0.045913	4.396008
225.269539	6636.178172	8.415181	-0.046005	4.398565
225.619157	6644.231204	8.420186	-0.046075	4.401146
225.475000	6652.184116	8.425190	-0.046053	4.403692
225.548193	6660.246368	8.430195	-0.046072	4.406272
225.967589	6668.214044	8.435200	-0.046155	4.408822
226.239003	6676.282675	8.440205	-0.046211	4.411402
226.316989	6684.323013	8.445210	-0.046231	4.413970
226.565208	6692.364448	8.450214	-0.046282	4.416538
226.822989	6700.353748	8.455219	-0.046335	4.419088
226.698337	6708.362383	8.460224	-0.046317	4.421641
226.985586	6716.338081	8.465229	-0.046376	4.424184
227.130515	6724.399038	8.470234	-0.046408	4.426752
227.237307	6732.405446	8.475238	-0.046433	4.429301
227.181306	6740.470888	8.480243	-0.046427	4.431866
227.401476	6748.472239	8.485248	-0.046473	4.434411
227.633134	6756.522350	8.490253	-0.046522	4.436970
227.681330	6764.473525	8.495258	-0.046536	4.439495
227.871765	6772.482424	8.500262	-0.046576	4.442037
228.087719	6780.468084	8.505267	-0.046622	4.444571
228.040411	6788.519995	8.510272	-0.046618	4.447123
228.169773	6796.552536	8.515277	-0.046647	4.449669
228.438298	6804.548499	8.520282	-0.046702	4.452202
228.575681	6812.602101	8.525286	-0.046733	4.454751
228.835722	6820.671691	8.530291	-0.046787	4.457304
228.609271	6828.581049	8.535296	-0.046750	4.459803
229.002521	6836.668201	8.540301	-0.046828	4.462359
229.030489	6844.642822	8.545306	-0.046838	4.464877
229.052910	6852.652706	8.550310	-0.046848	4.467405
229.440222	6860.707523	8.555315	-0.046925	4.469946
229.350670	6868.695173	8.560320	-0.046913	4.472464
229.624582	6876.723919	8.565325	-0.046969	4.474994
229.731750	6884.735330	8.570330	-0.046994	4.477516
229.900899	6892.717895	8.575335	-0.047031	4.480029
229.963976	6900.773655	8.580339	-0.047048	4.482562
230.301665	6908.739765	8.585344	-0.047116	4.485067
230.446806	6916.770076	8.590349	-0.047148	4.487590
230.560263	6924.803295	8.595354	-0.047174	4.490112
230.893445	6932.836960	8.600359	-0.047241	4.492634
231.068581	6940.867819	8.605363	-0.047279	4.495153
231.105499	6948.867677	8.610368	-0.047291	4.497660
231.086103	6956.871538	8.615373	-0.047293	4.500167
231.254743	6964.872198	8.620378	-0.047329	4.502672
231.581675	6972.894969	8.625383	-0.047395	4.505183
231.450480	6980.954227	8.630387	-0.047376	4.507703
231.591227	6988.922753	8.635392	-0.047407	4.510193
232.020680	6996.988373	8.640397	-0.047492	4.512714
232.156857	7005.035004	8.645402	-0.047523	4.515226
232.221366	7012.973628	8.650407	-0.047540	4.517703
232.460109	7020.990435	8.655411	-0.047590	4.520204
232.548016	7028.950767	8.660416	-0.047611	4.522685
232.558449	7036.980234	8.665421	-0.047618	4.525186
232.880014	7044.986903	8.670426	-0.047683	4.527679
232.758615	7053.009157	8.675431	-0.047666	4.530175
232.976921	7061.071716	8.680435	-0.047711	4.532682
233.101422	7069.093211	8.685440	-0.047740	4.535175
233.413535	7077.090868	8.690445	-0.047803	4.537660
233.358820	7085.103291	8.695450	-0.047798	4.540147
233.590754	7093.104336	8.700455	-0.047846	4.542630
233.871703	7101.150870	8.705459	-0.047904	4.545126
233.952507	7109.149627	8.710464	-0.047924	4.547605
234.044031	7117.176929	8.715469	-0.047946	4.550092
234.062079	7125.193904	8.720474	-0.047954	4.552574
234.234623	7133.209474	8.725479	-0.047992	4.555054
234.261037	7141.268541	8.730483	-0.048002	4.557547
234.099613	7149.236889	8.735488	-0.047977	4.560009
234.405547	7157.293426	8.740493	-0.048039	4.562499
234.820083	7165.234694	8.745498	-0.048121	4.564951
234.839964	7173.289204	8.750503	-0.048130	4.567436
234.999962	7181.326338	8.755507	-0.048165	4.569915
235.150667	7189.428726	8.760512	-0.048198	4.572413
235.347457	7197.410776	8.765517	-0.048240	4.574872
235.282102	7205.371645	8.770522	-0.048233	4.577323
235.314512	7213.349671	8.775527	-0.048244	4.579778
235.519414	7221.416821	8.780531	-0.048287	4.582260
235.581166	7229.387201	8.785536	-0.048304	4.584710
235.752503	7237.440905	8.790541	-0.048341	4.587184
235.909732	7245.453298	8.795546	-0.048375	4.589645
235.950668	7253.465195	8.800551	-0.048388	4.592104
236.142834	7261.548342	8.805555	-0.048429	4.594583
236.407808	7269.570634	8.810560	-0.048483	4.597043
236.288026	7277.497968	8.815565	-0.048466	4.599471
236.398773	7285.482214	8.820570	-0.048492	4.601917
236.613557	7293.465557	8.825575	-0.048537	4.604360
236.793118	7301.564529	8.830579	-0.048576	4.606838
236.757620	7309.550601	8.835584	-0.048574	4.609280
237.025885	7317.635828	8.840589	-0.048629	4.611750
237.272643	7325.630417	8.845594	-0.048680	4.614192
237.331895	7333.619111	8.850599	-0.048696	4.616631
237.204762	7341.640678	8.855603	-0.048678	4.619078
237.503261	7349.665608	8.860608	-0.048739	4.621525
237.684770	7357.627216	8.865613	-0.048777	4.623951
237.598491	7365.660534	8.870618	-0.048767	4.626398
237.896802	7373.671792	8.875623	-0.048827	4.628837
238.158706	7381.747906	8.880627	-0.048881	4.631295
238.166449	7389.790075	8.885632	-0.048888	4.633740
238.125926	7397.781976	8.890637	-0.048885	4.636170
238.249088	7405.737234	8.895642	-0.048913	4.638586
238.276739	7413.779813	8.900647	-0.048924	4.641028
238.553728	7421.790140	8.905651	-0.048980	4.643459
238.744143	7429.774719	8.910656	-0.049021	4.645881
238.774147	7437.818762	8.915661	-0.049032	4.648320
238.873189	7445.853840	8.920666	-0.049055	4.650754
239.258824	7453.848644	8.925671	-0.049132	4.653175
239.292431	7461.896188	8.930675	-0.049143	4.655611
239.466792	7469.849338	8.935680	-0.049181	4.658017
239.671151	7477.877010	8.940685	-0.049224	4.660444
239.837841	7485.940849	8.945690	-0.049260	4.662880
239.983554	7493.919981	8.950695	-0.049293	4.665290
240.228059	7502.012324	8.955699	-0.049343	4.667733
240.211658	7509.953673	8.960704	-0.049345	4.670129
240.330624	7518.044684	8.965709	-0.049373	4.672569
240.513703	7526.096763	8.970714	-0.049412	4.674996
240.545212	7534.047667	8.975719	-0.049423	4.677391
240.877176	7542.017675	8.980723	-0.049490	4.679790
240.658121	7550.036736	8.985728	-0.049454	4.682204
240.833165	7557.989337	8.990733	-0.049492	4.684595
240.915119	7566.078511	8.995738	-0.049512	4.687027
241.087300	7573.995774	9.000743	-0.049549	4.689406
241.226501	7582.129055	9.005747	-0.049580	4.691848
241.560538	7590.112837	9.010752	-0.049648	4.694244
241.638317	7598.144984	9.015757	-0.049667	4.696653
241.743224	7606.121070	9.020762	-0.049692	4.699045
241.848911	7614.151287	9.025767	-0.049717	4.701451
242.057037	7622.128005	9.030771	-0.049761	4.703840
242.066219	7630.192960	9.035776	-0.049767	4.706255
242.044325	7638.147044	9.040781	-0.049768	4.708635
242.292988	7646.226239	9.045786	-0.049820	4.711051
242.542542	7654.215672	9.050791	-0.049871	4.713439
242.688144	7662.294135	9.055795	-0.049904	4.715852
242.711210	7670.254491	9.060800	-0.049913	4.718229
242.976350	7678.266943	9.065805	-0.049968	4.720620
243.220062	7686.308507	9.070810	-0.050018	4.723018
243.056713	7694.280515	9.075815	-0.049993	4.725396
243.413532	7702.327165	9.080819	-0.050064	4.727793
243.591489	7710.360678	9.085824	-0.050103	4.730185
243.710795	7718.369464	9.090829	-0.050130	4.732569
243.661320	7726.441599	9.095834	-0.050126	4.734971
243.661029	7734.391250	9.100839	-0.050131	4.737335
244.093961	7742.405917	9.105843	-0.050217	4.739717
244.347622	7750.434532	9.110848	-0.050269	4.742101
244.468395	7758.391256	9.115853	-0.050297	4.744464
244.506793	7766.499483	9.120858	-0.050309	4.746870
244.455147	7774.450877	9.125863	-0.050304	4.749229
245.011257	7782.549763	9.130867	-0.050413	4.751629
244.933394	7790.536329	9.135872	-0.050404	4.753996
244.922393	7798.551858	9.140877	-0.050407	4.756370
245.046019	7806.539191	9.145882	-0.050435	4.758734
245.155386	7814.520887	9.150887	-0.050460	4.761096
245.514678	7822.542298	9.155891	-0.050532	4.763467
245.391382	7830.605330	9.160896	-0.050515	4.765851
245.752411	7838.556763	9.165901	-0.050587	4.768199
245.793604	7846.600268	9.170906	-0.050600	4.770574
245.733780	7854.620076	9.175911	-0.050594	4.772942
245.955533	7862.670760	9.180915	-0.050640	4.775316
246.238828	7870.645861	9.185920	-0.050698	4.777666
246.503417	7878.680914	9.190925	-0.050752	4.780033
246.513708	7886.720879	9.195930	-0.050759	4.782402
246.366450	7894.608904	9.200935	-0.050737	4.784725
246.696095	7902.732271	9.205939	-0.050804	4.787114
246.722205	7910.646424	9.210944	-0.050814	4.789442
246.797927	7918.764841	9.215949	-0.050833	4.791828
247.018808	7926.787414	9.220954	-0.050879	4.794185
247.032764	7934.790801	9.225959	-0.050887	4.796535
247.353431	7942.762246	9.230963	-0.050952	4.798874
247.342083	7950.809356	9.235968	-0.050955	4.801235
247.356947	7958.770321	9.240973	-0.050963	4.803570
247.401053	7966.842155	9.245978	-0.050976	4.805936
247.672287	7974.835197	9.250983	-0.051032	4.808276
247.731121	7982.890743	9.255987	-0.051048	4.810635
247.783358	7990.398579	9.260992	-0.051062	4.812832
248.007924	7995.070468	9.265997	-0.051107	4.814198

248.097765	7997.702755	9.271002	-0.051125	4.814968
248.096944	7998.992165	9.276007	-0.051126	4.815345
248.343322	7999.453020	9.281011	-0.051172	4.815478
248.266974	8000.509687	9.286016	-0.051158	4.815788
248.372377	8000.522063	9.291021	-0.051178	4.815791
248.459577	8000.533076	9.296026	-0.051194	4.815794
248.445997	8000.534982	9.301031	-0.051191	4.815794
248.563279	8000.559294	9.306035	-0.051213	4.815801
248.473810	8000.521537	9.311040	-0.051196	4.815790
248.676554	8000.582464	9.316045	-0.051234	4.815807
248.778326	8000.569160	9.321050	-0.051253	4.815803
248.891648	8000.549637	9.326055	-0.051274	4.815797
248.986819	8000.573591	9.331059	-0.051291	4.815803
248.790580	8000.546913	9.336064	-0.051255	4.815796
248.779879	8000.587298	9.341069	-0.051253	4.815808
248.739339	8000.574889	9.346074	-0.051245	4.815805
249.091946	8000.558179	9.351079	-0.051311	4.815798
249.229923	8000.582828	9.356083	-0.051336	4.815805
249.100984	8000.534822	9.361088	-0.051312	4.815791
249.249757	8000.551104	9.366093	-0.051340	4.815795
249.083139	8000.549460	9.371098	-0.051309	4.815796
249.072090	8000.547137	9.376103	-0.051306	4.815795
249.154204	8000.559136	9.381107	-0.051322	4.815798
249.143929	8000.560028	9.386112	-0.051320	4.815798
249.194015	8000.575778	9.391117	-0.051329	4.815803
249.297191	8000.580645	9.396122	-0.051348	4.815804
249.227386	8000.583774	9.401127	-0.051335	4.815805
249.336613	8000.484117	9.406131	-0.051355	4.815775
249.240705	8000.557283	9.411136	-0.051337	4.815797
249.375998	8000.592564	9.416141	-0.051362	4.815807
249.382313	8000.561697	9.421146	-0.051363	4.815798
249.236275	8000.518752	9.426151	-0.051336	4.815786
249.455574	8000.579949	9.431155	-0.051377	4.815803
249.628254	8000.569931	9.436160	-0.051409	4.815799
249.440062	8000.587153	9.441165	-0.051374	4.815805
249.429311	8000.559213	9.446170	-0.051371	4.815797
249.597703	8000.569408	9.451175	-0.051403	4.815799
249.513818	8000.597931	9.456179	-0.051387	4.815808
249.388879	8000.469921	9.461184	-0.051364	4.815771
249.485795	8000.571837	9.466189	-0.051382	4.815800
249.613248	8000.586707	9.471194	-0.051405	4.815804
249.621359	8000.559072	9.476199	-0.051407	4.815796
249.686288	8000.578265	9.481203	-0.051419	4.815801
249.793903	8000.550110	9.486208	-0.051439	4.815793
249.681513	8000.586711	9.491213	-0.051418	4.815804
249.634079	8000.560310	9.496218	-0.051409	4.815796
249.516704	8000.569073	9.501223	-0.051387	4.815799
249.517952	8000.511435	9.506227	-0.051387	4.815783
249.523410	8000.560623	9.511232	-0.051388	4.815797
249.736976	8000.590769	9.516237	-0.051427	4.815805
249.854104	8000.576647	9.521242	-0.051449	4.815800
249.667819	8000.535182	9.526247	-0.051414	4.815789
249.797559	8000.495642	9.531251	-0.051438	4.815777
249.952478	8000.567540	9.536256	-0.051467	4.815797
249.895150	8000.576209	9.541261	-0.051456	4.815800
249.761618	8000.560155	9.546266	-0.051431	4.815796
249.945148	8000.556719	9.551271	-0.051465	4.815794
249.990964	8000.594819	9.556275	-0.051474	4.815805
249.982695	8000.569054	9.561280	-0.051472	4.815797
250.051609	8000.497566	9.566285	-0.051485	4.815776
250.073684	8000.567309	9.571290	-0.051489	4.815796
249.927747	8000.585217	9.576295	-0.051462	4.815802
249.876769	8000.575840	9.581299	-0.051452	4.815800
249.985873	8000.548776	9.586304	-0.051472	4.815791
250.083387	8000.591986	9.591309	-0.051490	4.815803
250.072678	8000.485043	9.596314	-0.051488	4.815772
250.019074	8000.582384	9.601319	-0.051478	4.815801
250.039610	8000.597655	9.606323	-0.051482	4.815805
249.963951	8000.461901	9.611328	-0.051468	4.815766
250.291806	8000.503510	9.616333	-0.051529	4.815777
250.314869	8000.590351	9.621338	-0.051533	4.815802
250.060821	8000.590490	9.626343	-0.051485	4.815803
250.149791	8000.500111	9.631347	-0.051502	4.815776
250.090592	8000.579212	9.636352	-0.051491	4.815800
249.946978	8000.517087	9.641357	-0.051464	4.815782
250.199214	8000.419749	9.646362	-0.051511	4.815753
250.035815	8000.583634	9.651367	-0.051480	4.815801
250.123823	8000.520997	9.656371	-0.051496	4.815783
249.952865	8000.591879	9.661376	-0.051465	4.815804
249.962799	8000.619789	9.666381	-0.051466	4.815812
250.069208	8000.509408	9.671386	-0.051486	4.815779
250.261510	8000.596861	9.676391	-0.051522	4.815804
250.329320	8000.511476	9.681395	-0.051534	4.815779
250.180617	8000.585922	9.686400	-0.051506	4.815801
250.268228	8000.509399	9.691405	-0.051523	4.815779
250.125589	8000.595687	9.696410	-0.051496	4.815804
250.241047	8000.474777	9.701415	-0.051517	4.815769
250.460331	8000.495408	9.706419	-0.051558	4.815774
250.292905	8000.567415	9.711424	-0.051527	4.815795
250.201798	8000.496533	9.716429	-0.051510	4.815775
250.339300	8000.589502	9.721434	-0.051535	4.815802
250.347841	8000.551198	9.726439	-0.051537	4.815790
250.149761	8000.593882	9.731443	-0.051500	4.815804
250.130725	8000.567941	9.736448	-0.051496	4.815796
250.317484	8000.502636	9.741453	-0.051531	4.815776
250.427838	8000.515094	9.746458	-0.051551	4.815779
250.398634	8000.594682	9.751463	-0.051546	4.815803
250.649916	8000.515478	9.756467	-0.051592	4.815779
250.679935	8000.486063	9.761472	-0.051598	4.815770
250.307063	8000.587831	9.766477	-0.051528	4.815801
250.537566	8000.501884	9.771482	-0.051571	4.815775
250.516360	8000.586940	9.776487	-0.051567	4.815800
250.458594	8000.600940	9.781491	-0.051556	4.815804
250.422553	8000.575791	9.786496	-0.051549	4.815797
250.503947	8000.486356	9.791501	-0.051564	4.815771
250.483928	8000.606662	9.796506	-0.051561	4.815806
250.420357	8000.572526	9.801511	-0.051549	4.815796
250.551215	8000.497773	9.806515	-0.051573	4.815774
250.421150	8000.584265	9.811520	-0.051549	4.815800
250.511310	8000.498175	9.816525	-0.051565	4.815774
250.631065	8000.601533	9.821530	-0.051588	4.815804
250.467999	8000.573255	9.826535	-0.051557	4.815796
250.462604	8000.497358	9.831539	-0.051556	4.815774
250.591427	8000.577375	9.836544	-0.051580	4.815797
250.621361	8000.594934	9.841549	-0.051585	4.815802
250.693968	8000.516032	9.846554	-0.051599	4.815779
250.571035	8000.480933	9.851559	-0.051576	4.815769
250.594454	8000.608350	9.856563	-0.051580	4.815806
250.641905	8000.561068	9.861568	-0.051589	4.815792
250.455307	8000.482231	9.866573	-0.051554	4.815770
250.692716	8000.586430	9.871578	-0.051598	4.815799
250.752110	8000.570303	9.876583	-0.051609	4.815794
250.543172	8000.503914	9.881587	-0.051570	4.815776
250.657827	8000.560214	9.886592	-0.051591	4.815792
250.629487	8000.594977	9.891597	-0.051586	4.815802
250.795977	8000.572047	9.896602	-0.051617	4.815794
250.604645	8000.543310	9.901607	-0.051581	4.815787
250.770270	8000.512893	9.906611	-0.051612	4.815777
250.792932	8000.586918	9.911616	-0.051616	4.815799
250.503724	8000.512820	9.916621	-0.051562	4.815779
250.685906	8000.482672	9.921626	-0.051596	4.815769
250.677739	8000.555128	9.926631	-0.051594	4.815790
250.585726	8000.593128	9.931635	-0.051577	4.815802
250.795763	8000.591190	9.936640	-0.051616	4.815800
250.855991	8000.516358	9.941645	-0.051627	4.815778
250.808135	8000.610590	9.946650	-0.051618	4.815806
250.584917	8000.582403	9.951655	-0.051576	4.815798
250.699233	8000.480691	9.956659	-0.051597	4.815768
250.921261	8000.570762	9.961664	-0.051639	4.815793
250.747069	8000.585008	9.966669	-0.051606	4.815798
250.771276	8000.487171	9.971674	-0.051611	4.815770
250.726085	8000.561162	9.976679	-0.051602	4.815792
250.881295	8000.504953	9.981683	-0.051631	4.815774
250.835427	8000.585339	9.986688	-0.051622	4.815798
250.794198	8000.567579	9.991693	-0.051614	4.815793
250.911000	8000.452028	9.996698	-0.051636	4.815759
250.807319	8000.560301	10.001703	-0.051617	4.815791
250.893706	8000.586249	10.006707	-0.051633	4.815798
250.586430	8000.494777	10.011712	-0.051575	4.815773
250.714867	8000.512866	10.016717	-0.051599	4.815778
250.876447	8000.500533	10.021722	-0.051629	4.815773
250.867090	8000.606067	10.026727	-0.051627	4.815804
250.969360	8000.495618	10.031731	-0.051646	4.815771
250.706379	8000.570344	10.036736	-0.051597	4.815794
250.902082	8000.509454	10.041741	-0.051634	4.815776
250.807787	8000.600798	10.046746	-0.051616	4.815803
250.604122	8000.480046	10.051751	-0.051578	4.815769
250.541717	8000.607138	10.056755	-0.051566	4.815806
250.841050	8000.496685	10.061760	-0.051622	4.815772
250.816177	8000.589155	10.066765	-0.051617	4.815799
250.681571	8000.513296	10.071770	-0.051592	4.815778
250.676727	8000.564454	10.076775	-0.051591	4.815793
250.897074	8000.595779	10.081779	-0.051632	4.815801
250.767311	8000.558433	10.086784	-0.051608	4.815791
250.753799	8000.578489	10.091789	-0.051605	4.815797
251.161786	8000.473002	10.096794	-0.051681	4.815764
250.764435	8000.540210	10.101799	-0.051607	4.815785
250.943948	8000.583684	10.106803	-0.051640	4.815797
251.004547	8000.567577	10.111808	-0.051651	4.815792
250.741734	8000.512057	10.116813	-0.051602	4.815777
250.959698	8000.573237	10.121818	-0.051643	4.815794
250.856667	8000.533121	10.126823	-0.051623	4.815783
250.852473	8000.488205	10.131827	-0.051622	4.815770
250.746842	8000.532389	10.136832	-0.051603	4.815783
250.983367	8000.507393	10.141837	-0.051647	4.815775
251.170456	8000.497609	10.146842	-0.051681	4.815771
250.876586	8000.602796	10.151847	-0.051627	4.815803
251.009693	8000.521673	10.156851	-0.051651	4.815779
250.931041	8000.589783	10.161856	-0.051636	4.815799
250.970371	8000.497529	10.166861	-0.051644	4.815772
251.177197	8000.499809	10.171866	-0.051682	4.815772
250.965513	8000.574301	10.176871	-0.051643	4.815794
251.014870	8000.529186	10.181875	-0.051652	4.815781
250.937905	8000.489493	10.186880	-0.051637	4.815770
250.907597	8000.502871	10.191885	-0.051631	4.815774
250.947246	8000.596389	10.196890	-0.051639	4.815801
250.953082	8000.470496	10.201895	-0.051640	4.815764
250.873984	8000.590912	10.206899	-0.051625	4.815800
251.049044	8000.477373	10.211904	-0.051657	4.815766
250.841313	8000.612784	10.216909	-0.051619	4.815806
251.049014	8000.499775	10.221914	-0.051657	4.815772
251.016427	8000.602797	10.226919	-0.051651	4.815803
251.188538	8000.500954	10.231923	-0.051683	4.815772
250.974976	8000.580754	10.236928	-0.051643	4.815796
251.145736	8000.513053	10.241933	-0.051675	4.815776
251.345979	8000.502416	10.246938	-0.051712	4.815772
251.158426	8000.553811	10.251943	-0.051677	4.815788
251.195237	8000.447638	10.256947	-0.051684	4.815756
251.293167	8000.454556	10.261952	-0.051702	4.815758
251.261344	8000.563996	10.266957	-0.051696	4.815790
251.103966	8000.519795	10.271962	-0.051666	4.815778
251.083672	8000.501308	10.276967	-0.051663	4.815773
251.206923	8000.496893	10.281971	-0.051685	4.815771
251.276174	8000.590892	10.286976	-0.051698	4.815798
251.118190	8000.495435	10.291981	-0.051669	4.815771
250.989004	8000.502938	10.296986	-0.051644	4.815774
250.975196	8000.577439	10.301991	-0.051642	4.815795
251.145829	8000.516142	10.306995	-0.051673	4.815777
250.991175	8000.494406	10.312000	-0.051645	4.815771
250.888602	8000.495935	10.317005	-0.051625	4.815772
250.983459	8000.602093	10.322010	-0.051643	4.815803
250.966107	8000.588991	10.327015	-0.051640	4.815799
251.225854	8000.516329	10.332019	-0.051688	4.815776
251.022827	8000.587758	10.337024	-0.051650	4.815798
251.193886	8000.479493	10.342029	-0.051682	4.815766
251.371775	8000.515468	10.347034	-0.051715	4.815775
251.285874	8000.573852	10.352039	-0.051699	4.815793
251.338310	8000.412415	10.357043	-0.051708	4.815745
251.216733	8000.611146	10.362048	-0.051686	4.815804
251.307042	8000.497300	10.367053	-0.051702	4.815770
251.077350	8000.514915	10.372058	-0.051659	4.815777
251.142088	8000.491402	10.377063	-0.051671	4.815769
251.120942	8000.604218	10.382067	-0.051667	4.815803
251.256257	8000.483628	10.387072	-0.051692	4.815767
251.096372	8000.586719	10.392077	-0.051663	4.815798
251.029332	8000.518362	10.397082	-0.051650	4.815778
251.025157	8000.512947	10.402087	-0.051649	4.815776
251.085523	8000.406088	10.407091	-0.051660	4.815745
251.152620	8000.584394	10.412096	-0.051673	4.815797
250.960576	8000.511872	10.417101	-0.051637	4.815776
251.174999	8000.611430	10.422106	-0.051677	4.815804
251.085242	8000.491458	10.427111	-0.051660	4.815770
251.295231	8000.600552	10.432115	-0.051699	4.815801
251.099037	8000.493799	10.437120	-0.051662	4.815770
251.118077	8000.614741	10.442125	-0.051666	4.815806
251.143219	8000.511580	10.447130	-0.051670	4.815775
251.246429	8000.476947	10.452135	-0.051689	4.815765
251.126221	8000.516625	10.457139	-0.051667	4.815777
251.089735	8000.603569	10.462144	-0.051660	4.815803
251.209122	8000.512614	10.467149	-0.051682	4.815775
251.427924	8000.581283	10.472154	-0.051723	4.815794
251.216277	8000.518051	10.477159	-0.051683	4.815777
251.357076	8000.582250	10.482163	-0.051709	4.815795
251.374622	8000.464019	10.487168	-0.051712	4.815760
251.387378	8000.606212	10.492173	-0.051715	4.815802
251.165238	8000.494767	10.497178	-0.051673	4.815770
251.344063	8000.577733	10.502183	-0.051706	4.815794
251.567336	8000.506614	10.507187	-0.051748	4.815772
251.254024	8000.492978	10.512192	-0.051689	4.815769
251.192463	8000.595530	10.517197	-0.051678	4.815800
251.269143	8000.498544	10.522202	-0.051692	4.815771
251.196052	8000.579556	10.527207	-0.051678	4.815795
251.251677	8000.584720	10.532211	-0.051689	4.815796
251.305292	8000.468143	10.537216	-0.051698	4.815762
251.174317	8000.559959	10.542221	-0.051674	4.815789
251.071961	8000.611670	10.547226	-0.051655	4.815805
251.316404	8000.480040	10.552231	-0.051700	4.815765
251.269623	8000.581764	10.557235	-0.051691	4.815795
251.289703	8000.570338	10.562240	-0.051695	4.815792
251.321750	8000.440598	10.567245	-0.051701	4.815754
251.460390	8000.605120	10.572250	-0.051727	4.815801
251.299816	8000.568340	10.577255	-0.051697	4.815791
251.410181	8000.510335	10.582259	-0.051717	4.815774
251.511605	8000.469268	10.587264	-0.051736	4.815761
251.591980	8000.596544	10.592269	-0.051751	4.815798
251.495869	8000.592840	10.597274	-0.051733	4.815798
251.288391	8000.491241	10.602279	-0.051694	4.815769
251.338111	8000.514459	10.607283	-0.051703	4.815775
251.415303	8000.487945	10.612288	-0.051717	4.815767
251.261290	8000.605010	10.617293	-0.051689	4.815802
251.382523	8000.518356	10.622298	-0.051711	4.815776
251.144904	8000.465380	10.627303	-0.051667	4.815762
251.395550	8000.530294	10.632307	-0.051713	4.815780
251.567321	8000.495706	10.637312	-0.051745	4.815769
251.494690	8000.602349	10.642317	-0.051732	4.815800
251.504867	8000.508554	10.647322	-0.051733	4.815773
251.443385	8000.573740	10.652327	-0.051722	4.815792
251.477862	8000.535856	10.657331	-0.051728	4.815781
251.353746	8000.516750	10.662336	-0.051705	4.815776
251.268575	8000.583687	10.667341	-0.051689	4.815796
251.439619	8000.524532	10.672346	-0.051721	4.815778
251.547226	8000.513459	10.677351	-0.051741	4.815774
251.538860	8000.515449	10.682355	-0.051739	4.815775
251.447135	8000.523560	10.687360	-0.051722	4.815778
251.488951	8000.544515	10.692365	-0.051730	4.815784
251.358365	8000.585091	10.697370	-0.051705	4.815796
251.279593	8000.522949	10.702375	-0.051690	4.815778
251.440926	8000.468974	10.707379	-0.051720	4.815762
251.377970	8000.611006	10.712384	-0.051709	4.815803
251.383719	8000.494719	10.717389	-0.051709	4.815769
251.414483	8000.514426	10.722394	-0.051715	4.815775
251.359124	8000.566900	10.727399	-0.051705	4.815791
251.506363	8000.594905	10.732403	-0.051732	4.815798
251.520298	8000.595123	10.737408	-0.051734	4.815798
251.558850	8000.470826	10.742413	-0.051741	4.815762
251.539769	8000.607165	10.747418	-0.051738	4.815802
251.550575	8000.498433	10.752423	-0.051740	4.815770
251.552440	8000.518739	10.757427	-0.051740	4.815776
251.438849	8000.584147	10.762432	-0.051719	4.815795
251.458360	8000.563102	10.767437	-0.051722	4.815789
251.507558	8000.413356	10.772442	-0.051731	4.815745
251.367704	8000.572289	10.777447	-0.051705	4.815792
251.370546	8000.612896	10.782451	-0.051706	4.815804
251.474657	8000.507814	10.787456	-0.051725	4.815773
251.617544	8000.484502	10.792461	-0.051751	4.815765
251.648327	8000.476452	10.797466	-0.051757	4.815763
251.493015	8000.582820	10.802471	-0.051728	4.815795
251.393697	8000.597213	10.807475	-0.051709	4.815799
251.442601	8000.554225	10.812480	-0.051718	4.815787
251.410593	8000.484301	10.817485	-0.051712	4.815766
251.635597	8000.592573	10.822490	-0.051754	4.815797
251.462740	8000.554525	10.827495	-0.051722	4.815787
251.507647	8000.553110	10.832499	-0.051730	4.815786
251.654890	8000.505313	10.837504	-0.051757	4.815771
251.436945	8000.497496	10.842509	-0.051717	4.815770
251.667430	8000.521513	10.847514	-0.051760	4.815776
251.599590	8000.606882	10.852519	-0.051747	4.815801
251.627434	8000.398069	10.857523	-0.051752	4.815740
251.703422	8000.506056	10.862528	-0.051766	4.815771
251.592960	8000.605680	10.867533	-0.051745	4.815801
251.582160	8000.486988	10.872538	-0.051743	4.815766
251.561800	8000.540030	10.877543	-0.051739	4.815782
251.623824	8000.520743	10.882547	-0.051751	4.815776
251.553682	8000.582586	10.887552	-0.051738	4.815794
251.830247	8000.495250	10.892557	-0.051789	4.815768
251.798484	8000.595084	10.897562	-0.051783	4.815797
251.443170	8000.575427	10.902567	-0.051717	4.815793
251.500883	8000.522973	10.907571	-0.051727	4.815777
251.550150	8000.496006	10.912576	-0.051736	4.815769
251.469923	8000.587578	10.917581	-0.051721	4.815796
251.503343	8000.499499	10.922586	-0.051727	4.815770
251.565986	8000.588053	10.927591	-0.051739	4.815796
251.822828	8000.469436	10.932595	-0.051787	4.815760
251.718653	8000.539267	10.937600	-0.051767	4.815781
251.529349	8000.514832	10.942605	-0.051732	4.815775
251.726939	8000.581022	10.947610	-0.051769	4.815793
251.744870	8000.562086	10.952615	-0.051772	4.815788
251.866429	8000.517075	10.957619	-0.051794	4.815774
251.938199	8000.587628	10.962624	-0.051808	4.815794
251.910387	8000.576491	10.967629	-0.051802	4.815791
251.782477	8000.518888	10.972634	-0.051778	4.815775
251.586904	8000.563748	10.977639	-0.051742	4.815789
251.602250	8000.565056	10.982643	-0.051745	4.815789
251.635476	8000.480175	10.987648	-0.051751	4.815764
251.701019	8000.555965	10.992653	-0.051763	4.815786
251.824539	8000.594261	10.997658	-0.051786	4.815797
251.537352	8000.481759	11.002663	-0.051732	4.815765
251.647018	8000.600970	11.007667	-0.051753	4.815799
251.843581	8000.488848	11.012672	-0.051789	4.815766
251.767272	8000.576214	11.017677	-0.051775	4.815792
251.752723	8000.518316	11.022682	-0.051772	4.815775
251.823063	8000.600590	11.027687	-0.051785	4.815798
251.656872	8000.469766	11.032691	-0.051754	4.815761
251.580952	8000.595573	11.037696	-0.051740	4.815798
251.664645	8000.583044	11.042701	-0.051755	4.815794
251.760553	8000.471423	11.047706	-0.051773	4.815761
251.517631	8000.548610	11.052711	-0.051728	4.815785
251.637312	8000.561221	11.057715	-0.051750	4.815788
251.596356	8000.570156	11.062720	-0.051742	4.815791
251.594944	8000.584003	11.067725	-0.051742	4.815795
251.537507	8000.578791	11.072730	-0.051731	4.815793
251.612577	8000.447615	11.077735	-0.051745	4.815755
251.659898	8000.609587	11.082739	-0.051753	4.815802
251.627445	8000.554601	11.087744	-0.051747	4.815786
251.758072	8000.493723	11.092749	-0.051771	4.815768
251.829075	8000.596292	11.097754	-0.051785	4.815797
251.645212	8000.559134	11.102759	-0.051750	4.815787
251.801807	8000.451701	11.107763	-0.051779	4.815755
251.913206	8000.584820	11.112768	-0.051800	4.815793
251.825871	8000.588731	11.117773	-0.051784	4.815795
251.877001	8000.493465	11.122778	-0.051793	4.815767
251.905688	8000.575063	11.127783	-0.051798	4.815791
251.863734	8000.577575	11.132787	-0.051790	4.815792
251.791829	8000.507002	11.137792	-0.051777	4.815771
251.653437	8000.577346	11.142797	-0.051751	4.815793
251.810574	8000.494477	11.147802	-0.051780	4.815768
251.823158	8000.588625	11.152807	-0.051782	4.815795
251.985538	8000.407619	11.157811	-0.051812	4.815741
252.008613	8000.610836	11.162816	-0.051817	4.815801
251.819113	8000.477498	11.167821	-0.051781	4.815763
251.984735	8000.500463	11.172826	-0.051812	4.815769
252.037401	8000.602736	11.177831	-0.051822	4.815798
251.975379	8000.470400	11.182835	-0.051810	4.815760
251.810086	8000.584080	11.187840	-0.051779	4.815794
251.647787	8000.561151	11.192845	-0.051749	4.815788
252.120720	8000.500492	11.197850	-0.051837	4.815768
251.773334	8000.588795	11.202855	-0.051772	4.815795
251.749649	8000.513666	11.207859	-0.051768	4.815774
251.978095	8000.476796	11.212864	-0.051810	4.815762
252.021221	8000.587455	11.217869	-0.051818	4.815794
251.862832	8000.517613	11.222874	-0.051788	4.815774
251.716368	8000.603840	11.227879	-0.051761	4.815800
251.672511	8000.453650	11.232883	-0.051753	4.815756
251.773952	8000.602622	11.237888	-0.051772	4.815799
251.727412	8000.492958	11.242893	-0.051763	4.815768
251.821311	8000.491271	11.247898	-0.051780	4.815767
251.625990	8000.591651	11.252903	-0.051744	4.815797
251.721770	8000.516328	11.257907	-0.051761	4.815774
251.970721	8000.504346	11.262912	-0.051808	4.815770
251.808339	8000.497430	11.267917	-0.051777	4.815769
251.919225	8000.612392	11.272922	-0.051798	4.815802
251.998793	8000.468475	11.277927	-0.051812	4.815759
252.148742	8000.530689	11.282931	-0.051840	4.815777
251.814772	8000.483620	11.287936	-0.051778	4.815764
251.642739	8000.576905	11.292941	-0.051746	4.815793
252.172733	8000.523579	11.297946	-0.051844	4.815774
251.870086	8000.583782	11.302951	-0.051788	4.815793
251.971282	8000.495734	11.307955	-0.051807	4.815767
251.821828	8000.597927	11.312960	-0.051779	4.815798
251.794528	8000.492847	11.317965	-0.051774	4.815767
251.873188	8000.600879	11.322970	-0.051788	4.815798
251.818198	8000.495348	11.327975	-0.051778	4.815768
252.062961	8000.534546	11.332979	-0.051823	4.815778
251.906571	8000.514915	11.337984	-0.051794	4.815773
252.005238	8000.505832	11.342989	-0.051812	4.815770
252.026096	8000.518973	11.347994	-0.051816	4.815774
251.957866	8000.476219	11.352999	-0.051803	4.815762
252.019925	8000.589320	11.358003	-0.051815	4.815794
252.030311	8000.570262	11.363008	-0.051817	4.815789
251.824117	8000.476156	11.368013	-0.051778	4.815762
251.729889	8000.510917	11.373018	-0.051760	4.815773
251.734180	8000.586780	11.378023	-0.051761	4.815795
251.882823	8000.565696	11.383027	-0.051789	4.815788
251.997559	8000.501357	11.388032	-0.051810	4.815769
251.945683	8000.568834	11.393037	-0.051800	4.815789
251.946010	8000.527193	11.398042	-0.051800	4.815777
251.730943	8000.483122	11.403047	-0.051760	4.815765
251.871981	8000.516364	11.408051	-0.051786	4.815774
252.034374	8000.504045	11.413056	-0.051816	4.815769
252.070513	8000.604982	11.418061	-0.051823	4.815799
252.057004	8000.504395	11.423066	-0.051820	4.815769
251.811317	8000.600755	11.428071	-0.051775	4.815799
251.931966	8000.508753	11.433075	-0.051797	4.815771
252.117946	8000.516034	11.438080	-0.051831	4.815773
251.804170	8000.485307	11.443085	-0.051773	4.815765
252.140730	8000.614610	11.448090	-0.051836	4.815801
251.923866	8000.492571	11.453095	-0.051795	4.815767
252.037596	8000.491206	11.458099	-0.051816	4.815766
251.765532	8000.518809	11.463104	-0.051765	4.815775
251.933740	8000.514057	11.468109	-0.051797	4.815773
252.105590	8000.516839	11.473114	-0.051828	4.815773
252.056880	8000.518174	11.478119	-0.051819	4.815774
252.056728	8000.493607	11.483123	-0.051819	4.815766
251.887543	8000.514339	11.488128	-0.051788	4.815773
251.804146	8000.590914	11.493133	-0.051772	4.815796
252.285087	8000.420418	11.498138	-0.051861	4.815744
252.299797	8000.528480	11.503143	-0.051864	4.815775
252.212953	8000.579376	11.508147	-0.051848	4.815791
252.196562	8000.516109	11.513152	-0.051845	4.815772
252.042482	8000.525343	11.518157	-0.051816	4.815776
252.023015	8000.525018	11.523162	-0.051812	4.815776
252.111297	8000.496548	11.528167	-0.051828	4.815767
252.099831	8000.485677	11.533171	-0.051826	4.815764
252.013379	8000.387109	11.538176	-0.051810	4.815735
251.886417	8000.522764	11.543181	-0.051786	4.815776
251.918490	8000.422918	11.548186	-0.051792	4.815746
251.979704	8000.612876	11.553191	-0.051803	4.815802
252.025040	8000.421427	11.558195	-0.051812	4.815745
251.954985	8000.525977	11.563200	-0.051799	4.815776
252.012174	8000.495935	11.568205	-0.051809	4.815767
252.057525	8000.374952	11.573210	-0.051817	4.815732
252.026698	8000.529250	11.578215	-0.051812	4.815777
252.115850	8000.356664	11.583219	-0.051828	4.815726
252.178692	8000.560527	11.588224	-0.051840	4.815785
251.851835	8000.561616	11.593229	-0.051779	4.815787
252.084322	8000.403101	11.598234	-0.051822	4.815740
252.011991	8000.499073	11.603239	-0.051808	4.815768
252.199068	8000.417758	11.608243	-0.051843	4.815744
252.161204	8000.508951	11.613248	-0.051836	4.815770
251.967214	8000.498319	11.618253	-0.051800	4.815768
252.201419	8000.387875	11.623258	-0.051843	4.815735
251.997841	8000.392035	11.628263	-0.051805	4.815737
251.993667	8000.386620	11.633267	-0.051804	4.815735
252.274780	8000.534239	11.638272	-0.051857	4.815777
252.059413	8000.508313	11.643277	-0.051816	4.815771
252.172380	8000.522950	11.648282	-0.051837	4.815774
251.947155	8000.401844	11.653287	-0.051795	4.815740
251.933576	8000.530799	11.658291	-0.051793	4.815778
251.921920	8000.402484	11.663296	-0.051790	4.815740
252.109866	8000.529373	11.668301	-0.051825	4.815777
252.294978	8000.425605	11.673306	-0.051860	4.815745
252.099353	8000.530252	11.678311	-0.051823	4.815777
251.969564	8000.380802	11.683315	-0.051799	4.815734
252.200064	8000.393076	11.688320	-0.051842	4.815736
252.132063	8000.599086	11.693325	-0.051829	4.815797
252.122869	8000.411022	11.698330	-0.051827	4.815742
252.130577	8000.513632	11.703335	-0.051828	4.815772
252.124355	8000.501778	11.708339	-0.051827	4.815769
251.919138	8000.495234	11.713344	-0.051789	4.815768
251.991039	8000.506002	11.718349	-0.051802	4.815770
251.997208	8000.419614	11.723354	-0.051803	4.815745
252.016023	8000.499984	11.728359	-0.051807	4.815769
252.134083	8000.601183	11.733363	-0.051828	4.815798
252.213588	8000.475415	11.738368	-0.051843	4.815760
252.142596	8000.540447	11.743373	-0.051830	4.815780
252.338149	8000.440052	11.748378	-0.051866	4.815749
252.310503	8000.523938	11.753383	-0.051861	4.815774
252.273615	8000.538277	11.758387	-0.051854	4.815779
252.125650	8000.529460	11.763392	-0.051826	4.815777
252.289037	8000.517157	11.768397	-0.051857	4.815772
252.360115	8000.441432	11.773402	-0.051870	4.815750
252.181016	8000.495100	11.778407	-0.051836	4.815766
252.175487	8000.524895	11.783411	-0.051835	4.815775
252.342294	8000.418695	11.788416	-0.051866	4.815743
252.340751	8000.484855	11.793421	-0.051866	4.815763
252.227167	8000.465920	11.798426	-0.051844	4.815758
252.268934	8000.478333	11.803431	-0.051852	4.815761
252.080191	8000.510492	11.808435	-0.051817	4.815771
252.149061	8000.511601	11.813440	-0.051830	4.815771
252.056617	8000.530376	11.818445	-0.051812	4.815777
252.198107	8000.389601	11.823450	-0.051838	4.815735
251.993373	8000.364916	11.828455	-0.051800	4.815729
251.933426	8000.523011	11.833459	-0.051789	4.815776
252.154742	8000.419832	11.838464	-0.051830	4.815744
252.060844	8000.517589	11.843469	-0.051813	4.815774
252.137811	8000.405660	11.848474	-0.051827	4.815740
252.088173	8000.387763	11.853479	-0.051817	4.815735
252.168970	8000.424298	11.858483	-0.051832	4.815746
252.230302	8000.415676	11.863488	-0.051844	4.815743
252.116838	8000.504574	11.868493	-0.051822	4.815769
252.408856	8000.538134	11.873498	-0.051877	4.815778
252.115502	8000.510941	11.878503	-0.051822	4.815771
252.143381	8000.494302	11.883507	-0.051827	4.815766
252.178445	8000.483118	11.888512	-0.051833	4.815763
252.057100	8000.608189	11.893517	-0.051811	4.815800
252.168534	8000.424219	11.898522	-0.051831	4.815746
252.218786	8000.587308	11.903527	-0.051841	4.815793
252.208395	8000.524140	11.908531	-0.051839	4.815775
252.179939	8000.472422	11.913536	-0.051833	4.815760
252.134164	8000.496225	11.918541	-0.051825	4.815767
252.362855	8000.291740	11.923546	-0.051867	4.815706
252.316426	8000.509844	11.928551	-0.051858	4.815770
252.064212	8000.420328	11.933555	-0.051811	4.815745
251.998126	8000.401097	11.938560	-0.051799	4.815740
252.069706	8000.511149	11.943565	-0.051812	4.815772
252.214445	8000.504949	11.948570	-0.051839	4.815769
252.193265	8000.507799	11.953575	-0.051835	4.815770
252.217479	8000.407825	11.958579	-0.051839	4.815741
252.257288	8000.291023	11.963584	-0.051847	4.815706
252.127699	8000.533399	11.968589	-0.051822	4.815778
251.980302	8000.392204	11.973594	-0.051795	4.815737
251.990225	8000.483105	11.978599	-0.051797	4.815764
251.942357	8000.468440	11.983603	-0.051788	4.815760
252.253574	8000.495904	11.988608	-0.051845	4.815766
252.155899	8000.504986	11.993613	-0.051827	4.815769
252.220064	8000.495342	11.998618	-0.051839	4.815766
252.340874	8000.469536	12.003623	-0.051861	4.815758
252.303642	8000.395256	12.008627	-0.051854	4.815737
252.077408	8000.420400	12.013632	-0.051812	4.815745
251.883135	8000.513324	12.018637	-0.051776	4.815773
252.141052	8000.491880	12.023642	-0.051824	4.815766
252.077931	8000.598678	12.028647	-0.051812	4.815797
252.050755	8000.585416	12.033651	-0.051807	4.815793
252.088914	8000.513427	12.038656	-0.051814	4.815772
252.212879	8000.499416	12.043661	-0.051837	4.815768
252.153137	8000.501640	12.048666	-0.051826	4.815769
252.228201	8000.604277	12.053671	-0.051839	4.815798
252.226810	8000.522036	12.058675	-0.051839	4.815774
252.365404	8000.527481	12.063680	-0.051865	4.815775
252.200306	8000.510912	12.068685	-0.051834	4.815771
252.348083	8000.407606	12.073690	-0.051861	4.815740
252.179767	8000.606649	12.078695	-0.051830	4.815799
252.042239	8000.505116	12.083699	-0.051804	4.815770
252.169115	8000.407876	12.088704	-0.051828	4.815741
252.125432	8000.529937	12.093709	-0.051819	4.815777
252.304482	8000.533903	12.098714	-0.051853	4.815777
252.294633	8000.480352	12.103719	-0.051851	4.815762
252.449935	8000.615254	12.108723	-0.051880	4.815800
252.498938	8000.431337	12.113728	-0.051889	4.815746
252.239727	8000.611822	12.118733	-0.051840	4.815800
252.105997	8000.502877	12.123738	-0.051815	4.815769
252.329578	8000.575895	12.128743	-0.051857	4.815789
252.221730	8000.504738	12.133747	-0.051837	4.815769
252.228331	8000.601992	12.138752	-0.051838	4.815798
252.069163	8000.485161	12.143757	-0.051808	4.815764
252.439558	8000.408957	12.148762	-0.051877	4.815740
252.404116	8000.459620	12.153767	-0.051870	4.815755
252.137531	8000.433930	12.158771	-0.051820	4.815749
252.369547	8000.604241	12.163776	-0.051864	4.815798
252.118089	8000.583066	12.168781	-0.051817	4.815793
252.148412	8000.526964	12.173786	-0.051822	4.815776
252.290026	8000.590111	12.178791	-0.051848	4.815794
252.289717	8000.498279	12.183795	-0.051848	4.815767
252.443438	8000.500767	12.188800	-0.051877	4.815767
252.346037	8000.596332	12.193805	-0.051859	4.815795
252.277114	8000.496980	12.198810	-0.051846	4.815767
252.105819	8000.596684	12.203815	-0.051814	4.815797
252.080315	8000.502308	12.208819	-0.051809	4.815769
252.186736	8000.568086	12.213824	-0.051828	4.815788
252.230199	8000.530348	12.218829	-0.051836	4.815777
252.164794	8000.518600	12.223834	-0.051824	4.815774
252.234431	8000.599796	12.228839	-0.051837	4.815797
252.256965	8000.500862	12.233843	-0.051841	4.815768
252.213604	8000.605846	12.238848	-0.051833	4.815799
252.292698	8000.507830	12.243853	-0.051848	4.815770
252.281259	8000.519379	12.248858	-0.051845	4.815773
252.423618	8000.594283	12.253863	-0.051872	4.815794
252.455591	8000.508313	12.258867	-0.051878	4.815769
252.527944	8000.494532	12.263872	-0.051891	4.815765
252.196089	8000.576681	12.268877	-0.051829	4.815790
252.234783	8000.516445	12.273882	-0.051836	4.815773
252.476107	8000.595091	12.278887	-0.051881	4.815794
252.297625	8000.509974	12.283891	-0.051848	4.815770
252.408413	8000.510696	12.288896	-0.051868	4.815770
252.401772	8000.581045	12.293901	-0.051867	4.815791
252.292451	8000.556840	12.298906	-0.051846	4.815784
252.114265	8000.574223	12.303911	-0.051813	4.815790
252.303824	8000.569818	12.308915	-0.051848	4.815788
252.460699	8000.516839	12.313920	-0.051877	4.815772
252.563920	8000.508898	12.318925	-0.051897	4.815769
252.429356	8000.540868	12.323930	-0.051871	4.815779
252.408898	8000.494618	12.328935	-0.051867	4.815765
252.287657	8000.500114	12.333939	-0.051845	4.815768
252.546514	8000.539541	12.338944	-0.051893	4.815778
252.358628	8000.581323	12.343949	-0.051858	4.815791
252.466287	8000.525409	12.348954	-0.051878	4.815774
252.363796	8000.503450	12.353959	-0.051859	4.815768
252.172703	8000.593224	12.358963	-0.051823	4.815795
252.337168	8000.505135	12.363968	-0.051853	4.815769
252.173174	8000.465096	12.368973	-0.051823	4.815758
252.210963	8000.625848	12.373978	-0.051830	4.815805
252.272545	8000.403701	12.378983	-0.051841	4.815739
252.180076	8000.519631	12.383987	-0.051824	4.815774
252.179060	8000.524944	12.388992	-0.051823	4.815775
252.289942	8000.596133	12.393997	-0.051844	4.815796
252.497729	8000.503410	12.399002	-0.051883	4.815768
252.377993	8000.513201	12.404007	-0.051860	4.815771
252.246052	8000.514252	12.409011	-0.051835	4.815772
252.547876	8000.613098	12.414016	-0.051892	4.815799
252.347228	8000.513742	12.419021	-0.051854	4.815771
252.279204	8000.524373	12.424026	-0.051841	4.815775
252.369229	8000.446820	12.429031	-0.051858	4.815752
252.444494	8000.559069	12.434035	-0.051872	4.815784
252.467740	8000.601076	12.439040	-0.051876	4.815796
252.398451	8000.464350	12.444045	-0.051863	4.815757
252.389565	8000.614735	12.449050	-0.051861	4.815801
252.415310	8000.511582	12.454055	-0.051866	4.815770
252.581516	8000.517476	12.459059	-0.051897	4.815771
252.454219	8000.464152	12.464064	-0.051873	4.815756
252.473023	8000.547725	12.469069	-0.051877	4.815781
252.362613	8000.527773	12.474074	-0.051856	4.815775
252.433230	8000.583362	12.479079	-0.051869	4.815791
252.427891	8000.521342	12.484083	-0.051868	4.815773
252.385237	8000.618865	12.489088	-0.051860	4.815802
252.440544	8000.490568	12.494093	-0.051870	4.815764
252.567716	8000.540669	12.499098	-0.051894	4.815778
252.495954	8000.623839	12.504103	-0.051880	4.815803
252.441365	8000.501231	12.509107	-0.051870	4.815767
252.455045	8000.596465	12.514112	-0.051872	4.815795
252.278585	8000.555155	12.519117	-0.051839	4.815784
252.326583	8000.531370	12.524122	-0.051848	4.815777
252.350742	8000.529618	12.529127	-0.051853	4.815776
252.537422	8000.524100	12.534131	-0.051887	4.815774
252.367739	8000.507456	12.539136	-0.051855	4.815769
252.323869	8000.563320	12.544141	-0.051847	4.815786
252.400313	8000.600852	12.549146	-0.051861	4.815797
252.351697	8000.515710	12.554151	-0.051852	4.815772
252.174811	8000.603578	12.559155	-0.051819	4.815798
252.276197	8000.513398	12.564160	-0.051838	4.815772
252.421839	8000.571272	12.569165	-0.051865	4.815788
252.543937	8000.619155	12.574170	-0.051888	4.815801
252.578312	8000.490519	12.579175	-0.051894	4.815764
252.441986	8000.591858	12.584179	-0.051868	4.815794
252.344677	8000.511263	12.589184	-0.051850	4.815771
252.483159	8000.571156	12.594189	-0.051876	4.815788
252.668791	8000.513305	12.599194	-0.051910	4.815770
252.605446	8000.609425	12.604199	-0.051898	4.815798
252.277171	8000.559243	12.609203	-0.051837	4.815785
252.728693	8000.477951	12.614208	-0.051921	4.815759
252.588063	8000.573883	12.619213	-0.051895	4.815788
252.606482	8000.603000	12.624218	-0.051898	4.815796
252.484656	8000.483570	12.629223	-0.051875	4.815762
252.433309	8000.609778	12.634227	-0.051866	4.815799
252.522581	8000.395554	12.639232	-0.051882	4.815736
252.322784	8000.606898	12.644237	-0.051845	4.815799
252.451917	8000.426418	12.649242	-0.051869	4.815745
252.538664	8000.581559	12.654247	-0.051885	4.815790
252.419799	8000.521967	12.659251	-0.051863	4.815774
252.455840	8000.418982	12.664256	-0.051869	4.815743
252.448399	8000.516008	12.669261	-0.051868	4.815772
252.489997	8000.524148	12.674266	-0.051876	4.815774
252.467331	8000.494944	12.679271	-0.051871	4.815765
252.524374	8000.372015	12.684275	-0.051882	4.815729
252.633025	8000.451708	12.689280	-0.051902	4.815752
252.529759	8000.396640	12.694285	-0.051882	4.815736
252.556055	8000.383179	12.699290	-0.051887	4.815732
252.645006	8000.410238	12.704295	-0.051904	4.815740
252.495930	8000.591444	12.709299	-0.051876	4.815793
252.490950	8000.516618	12.714304	-0.051875	4.815772
252.402732	8000.488486	12.719309	-0.051858	4.815764
252.518408	8000.597121	12.724314	-0.051880	4.815795
252.370790	8000.496491	12.729319	-0.051852	4.815766
252.309461	8000.502959	12.734323	-0.051841	4.815769
252.554066	8000.355317	12.739328	-0.051886	4.815724
252.445094	8000.598030	12.744333	-0.051866	4.815796
252.422255	8000.498358	12.749338	-0.051861	4.815767
252.476376	8000.596385	12.754343	-0.051871	4.815795
252.540373	8000.574994	12.759347	-0.051883	4.815789
252.487550	8000.419318	12.764352	-0.051873	4.815743
252.393648	8000.577932	12.769357	-0.051856	4.815790
252.460421	8000.511745	12.774362	-0.051868	4.815770
252.564244	8000.481393	12.779367	-0.051887	4.815761
252.532859	8000.630346	12.784371	-0.051881	4.815805
252.509522	8000.426037	12.789376	-0.051877	4.815745
252.357175	8000.531386	12.794381	-0.051848	4.815777
252.655753	8000.524482	12.799386	-0.051904	4.815773
252.593156	8000.526659	12.804391	-0.051892	4.815774
252.321792	8000.504094	12.809395	-0.051841	4.815769
252.481254	8000.625184	12.814400	-0.051871	4.815803
252.409513	8000.485215	12.819405	-0.051858	4.815763
252.640980	8000.625625	12.824410	-0.051901	4.815803
252.457113	8000.514797	12.829415	-0.051866	4.815771
252.687119	8000.511049	12.834419	-0.051909	4.815769
252.921791	8000.431575	12.839424	-0.051952	4.815745
252.620972	8000.598573	12.844429	-0.051896	4.815795
252.496681	8000.525012	12.849434	-0.051873	4.815774
252.454153	8000.518975	12.854439	-0.051865	4.815773
252.484817	8000.567508	12.859443	-0.051871	4.815787
252.465788	8000.509537	12.864448	-0.051867	4.815770
252.349263	8000.582371	12.869453	-0.051845	4.815792
252.459448	8000.530769	12.874458	-0.051866	4.815776
252.529736	8000.485993	12.879463	-0.051879	4.815763
252.459321	8000.580929	12.884467	-0.051866	4.815791
252.724940	8000.529716	12.889472	-0.051915	4.815774
252.565489	8000.501494	12.894477	-0.051885	4.815767
252.476339	8000.612141	12.899482	-0.051868	4.815800
252.671559	8000.494657	12.904487	-0.051905	4.815764
252.631637	8000.605036	12.909491	-0.051897	4.815797
252.534134	8000.527640	12.914496	-0.051879	4.815775
252.677874	8000.500071	12.919501	-0.051905	4.815766
252.766912	8000.569839	12.924506	-0.051922	4.815786
252.696979	8000.489687	12.929511	-0.051909	4.815763
252.514819	8000.602027	12.934515	-0.051875	4.815797
252.917556	8000.499658	12.939520	-0.051950	4.815765
252.698788	8000.599659	12.944525	-0.051909	4.815795
252.438786	8000.512150	12.949530	-0.051860	4.815771
252.702444	8000.571941	12.954535	-0.051909	4.815787
252.652256	8000.516667	12.959539	-0.051900	4.815771
252.558309	8000.613356	12.964544	-0.051882	4.815800
252.454271	8000.546531	12.969549	-0.051863	4.815781
252.832784	8000.553737	12.974554	-0.051933	4.815781
252.787098	8000.484656	12.979559	-0.051925	4.815761
252.709086	8000.571996	12.984563	-0.051910	4.815787
252.802569	8000.539340	12.989568	-0.051927	4.815777
252.593411	8000.498566	12.994573	-0.051888	4.815766
252.755466	8000.522542	12.999578	-0.051918	4.815772
252.824669	8000.495898	13.004583	-0.051931	4.815764
252.652670	8000.527261	13.009587	-0.051899	4.815774
252.644565	8000.499361	13.014592	-0.051897	4.815766
252.558698	8000.607926	13.019597	-0.051881	4.815798
252.691880	8000.475556	13.024602	-0.051906	4.815759
252.371150	8000.589915	13.029607	-0.051846	4.815794
252.338384	8000.572292	13.034611	-0.051840	4.815789
252.564752	8000.485209	13.039616	-0.051882	4.815762
252.557610	8000.556617	13.044621	-0.051881	4.815783
252.469579	8000.572261	13.049626	-0.051864	4.815788
252.494041	8000.581190	13.054631	-0.051869	4.815791
252.508974	8000.460779	13.059635	-0.051871	4.815755
252.452949	8000.606129	13.064640	-0.051861	4.815798
252.522802	8000.565616	13.069645	-0.051874	4.815786
252.572739	8000.497020	13.074650	-0.051883	4.815766
252.772256	8000.596341	13.079655	-0.051920	4.815794
252.481016	8000.586264	13.084659	-0.051866	4.815792
252.743095	8000.528587	13.089664	-0.051914	4.815774
252.736244	8000.531670	13.094669	-0.051913	4.815775
252.729667	8000.576396	13.099674	-0.051911	4.815788
252.672776	8000.587207	13.104679	-0.051901	4.815792
252.515196	8000.466130	13.109683	-0.051871	4.815757
252.446518	8000.618747	13.114688	-0.051858	4.815802
252.555486	8000.450751	13.119693	-0.051879	4.815752
252.564530	8000.590752	13.124698	-0.051880	4.815793
252.617955	8000.558513	13.129703	-0.051890	4.815784
252.493084	8000.575694	13.134707	-0.051867	4.815789
252.430699	8000.531966	13.139712	-0.051855	4.815777
252.504838	8000.464831	13.144717	-0.051869	4.815757
252.526538	8000.581549	13.149722	-0.051873	4.815791
252.545993	8000.501782	13.154727	-0.051876	4.815767
252.655254	8000.571877	13.159731	-0.051896	4.815787
252.862065	8000.578430	13.164736	-0.051935	4.815788
252.767511	8000.556600	13.169741	-0.051917	4.815782
252.872237	8000.575375	13.174746	-0.051937	4.815787
252.926926	8000.488706	13.179751	-0.051947	4.815762
252.753243	8000.574492	13.184755	-0.051914	4.815788
252.824904	8000.489167	13.189760	-0.051927	4.815762
252.775858	8000.579112	13.194765	-0.051918	4.815789
252.688002	8000.507211	13.199770	-0.051902	4.815768
252.608029	8000.608398	13.204775	-0.051887	4.815798
252.643224	8000.507534	13.209779	-0.051893	4.815769
252.637931	8000.612069	13.214784	-0.051892	4.815799
252.530787	8000.586832	13.219789	-0.051872	4.815792
252.657072	8000.463958	13.224794	-0.051895	4.815756
252.764736	8000.601290	13.229799	-0.051915	4.815795
252.735416	8000.594399	13.234803	-0.051910	4.815793
252.825725	8000.525391	13.239808	-0.051926	4.815773
252.735475	8000.501496	13.244813	-0.051910	4.815766
252.595556	8000.611318	13.249818	-0.051883	4.815799
252.740444	8000.442838	13.254823	-0.051910	4.815749
252.775195	8000.573647	13.259827	-0.051917	4.815787
252.912468	8000.507538	13.264832	-0.051942	4.815767
252.741262	8000.589093	13.269837	-0.051910	4.815792
252.586601	8000.494754	13.274842	-0.051881	4.815765
252.844844	8000.604638	13.279847	-0.051929	4.815796
252.784952	8000.604723	13.284851	-0.051918	4.815796
252.723750	8000.410475	13.289856	-0.051906	4.815740
252.923743	8000.620840	13.294861	-0.051944	4.815800
252.630684	8000.524252	13.299866	-0.051889	4.815774
252.722547	8000.512923	13.304871	-0.051906	4.815770
252.811801	8000.498349	13.309875	-0.051922	4.815765
252.757152	8000.527347	13.314880	-0.051912	4.815774
252.552119	8000.558173	13.319885	-0.051874	4.815784
252.591094	8000.552391	13.324890	-0.051881	4.815782
252.801610	8000.593170	13.329895	-0.051920	4.815793
252.669160	8000.485312	13.334899	-0.051895	4.815762
252.768766	8000.514679	13.339904	-0.051914	4.815770
252.790998	8000.584429	13.344909	-0.051918	4.815790
252.811369	8000.512150	13.349914	-0.051922	4.815769
252.602598	8000.600569	13.354919	-0.051883	4.815796
252.651482	8000.458289	13.359923	-0.051892	4.815754
252.767113	8000.572261	13.364928	-0.051913	4.815787
252.643828	8000.473094	13.369933	-0.051890	4.815759
252.870893	8000.516276	13.374938	-0.051932	4.815770
252.797757	8000.520417	13.379943	-0.051918	4.815772
252.557714	8000.546404	13.384947	-0.051874	4.815780
252.542993	8000.619824	13.389952	-0.051871	4.815802
252.691175	8000.498374	13.394957	-0.051898	4.815766
252.723440	8000.530919	13.399962	-0.051904	4.815775
252.657796	8000.520235	13.404967	-0.051892	4.815772
252.877200	8000.506707	13.409971	-0.051933	4.815767
252.960874	8000.521937	13.414976	-0.051948	4.815771
252.833911	8000.500648	13.419981	-0.051924	4.815766
252.734282	8000.513968	13.424986	-0.051906	4.815770
252.917793	8000.523345	13.429991	-0.051940	4.815772
252.669516	8000.521440	13.434995	-0.051893	4.815773
252.692298	8000.508989	13.440000	-0.051898	4.815769
252.750311	8000.617756	13.445005	-0.051908	4.815800
252.676691	8000.512988	13.450010	-0.051894	4.815770
252.716112	8000.507214	13.455015	-0.051902	4.815768
252.681725	8000.518390	13.460019	-0.051895	4.815772
252.893446	8000.536767	13.465024	-0.051935	4.815776
252.774633	8000.492122	13.470029	-0.051912	4.815764
252.821449	8000.611384	13.475034	-0.051921	4.815798
252.748762	8000.502361	13.480039	-0.051907	4.815767
252.767304	8000.593404	13.485043	-0.051911	4.815793
252.935859	8000.511788	13.490048	-0.051942	4.815769
252.908280	8000.576458	13.495053	-0.051937	4.815788
252.899696	8000.468476	13.500058	-0.051935	4.815756
252.895435	8000.592247	13.505063	-0.051934	4.815792
252.878507	8000.593031	13.510067	-0.051931	4.815793
253.036699	8000.522990	13.515072	-0.051960	4.815771
252.715831	8000.579694	13.520077	-0.051900	4.815789
252.779053	8000.599930	13.525082	-0.051912	4.815795
252.733884	8000.518045	13.530087	-0.051903	4.815771
252.663517	8000.584156	13.535091	-0.051890	4.815791
252.616742	8000.511854	13.540096	-0.051881	4.815770
252.517002	8000.602044	13.545101	-0.051863	4.815797
252.663152	8000.567041	13.550106	-0.051890	4.815786
252.720480	8000.512445	13.555111	-0.051900	4.815770
252.703715	8000.526043	13.560115	-0.051897	4.815774
252.833942	8000.594344	13.565120	-0.051921	4.815793
252.635491	8000.570826	13.570125	-0.051884	4.815787
252.606635	8000.521237	13.575130	-0.051879	4.815773
252.808539	8000.485004	13.580135	-0.051916	4.815761
252.668077	8000.525420	13.585139	-0.051890	4.815774
252.850376	8000.581755	13.590144	-0.051924	4.815789
252.721380	8000.564703	13.595149	-0.051900	4.815785
252.751063	8000.519267	13.600154	-0.051905	4.815772
252.666572	8000.526427	13.605159	-0.051889	4.815774
252.601397	8000.599028	13.610163	-0.051877	4.815796
252.869440	8000.521163	13.615168	-0.051927	4.815772
252.797131	8000.491153	13.620173	-0.051913	4.815763
252.566028	8000.589886	13.625178	-0.051870	4.815793
252.781911	8000.594451	13.630183	-0.051910	4.815793
252.799666	8000.461273	13.635187	-0.051914	4.815754
252.672018	8000.605460	13.640192	-0.051890	4.815797
252.724429	8000.593491	13.645197	-0.051899	4.815793
252.864033	8000.504998	13.650202	-0.051925	4.815767
252.982703	8000.596600	13.655207	-0.051947	4.815793
252.694752	8000.477675	13.660211	-0.051893	4.815760
252.770774	8000.583531	13.665216	-0.051908	4.815790
252.809813	8000.559600	13.670221	-0.051915	4.815783
252.947097	8000.587445	13.675226	-0.051940	4.815791
252.866697	8000.533815	13.680231	-0.051925	4.815775
252.818410	8000.496721	13.685235	-0.051916	4.815765
252.875068	8000.506174	13.690240	-0.051926	4.815767
252.726826	8000.583832	13.695245	-0.051899	4.815791
252.742710	8000.618246	13.700250	-0.051902	4.815801
252.695041	8000.509629	13.705255	-0.051893	4.815769
252.590113	8000.569840	13.710259	-0.051873	4.815787
252.735590	8000.540164	13.715264	-0.051900	4.815778
252.760792	8000.509603	13.720269	-0.051905	4.815769
252.615327	8000.527517	13.725274	-0.051877	4.815775
252.846976	8000.473617	13.730279	-0.051920	4.815758
252.896965	8000.532073	13.735283	-0.051930	4.815775
252.879471	8000.529645	13.740288	-0.051926	4.815774
252.916650	8000.498210	13.745293	-0.051933	4.815765
253.134014	8000.520949	13.750298	-0.051973	4.815770
252.984357	8000.523848	13.755303	-0.051946	4.815772
252.719412	8000.576122	13.760307	-0.051896	4.815789
252.903937	8000.617546	13.765312	-0.051930	4.815800
252.798645	8000.474896	13.770317	-0.051911	4.815759
252.807449	8000.518804	13.775322	-0.051912	4.815771
252.740241	8000.528380	13.780327	-0.051900	4.815774
252.591695	8000.498200	13.785331	-0.051872	4.815766
252.781849	8000.525835	13.790336	-0.051907	4.815774
252.808586	8000.588184	13.795341	-0.051912	4.815792
252.712662	8000.538573	13.800346	-0.051894	4.815778
252.935614	8000.506952	13.805351	-0.051935	4.815767
252.803180	8000.581664	13.810355	-0.051911	4.815790
252.744455	8000.510236	13.815360	-0.051900	4.815769
252.788977	8000.603836	13.820365	-0.051908	4.815796
252.899661	8000.589610	13.825370	-0.051928	4.815792
252.973720	8000.515000	13.830375	-0.051942	4.815769
252.938256	8000.601964	13.835379	-0.051935	4.815795
252.973866	8000.599330	13.840384	-0.051942	4.815794
252.766879	8000.492397	13.845389	-0.051903	4.815764
252.768198	8000.578889	13.850394	-0.051903	4.815789
252.988740	8000.517335	13.855399	-0.051944	4.815770
252.662247	8000.579286	13.860403	-0.051883	4.815790
252.755756	8000.501789	13.865408	-0.051901	4.815767
252.929326	8000.431999	13.870413	-0.051933	4.815745
252.815020	8000.521952	13.875418	-0.051912	4.815772
252.905408	8000.497787	13.880423	-0.051928	4.815765
252.906739	8000.596024	13.885427	-0.051928	4.815793
253.108213	8000.503198	13.890432	-0.051966	4.815765
252.928800	8000.571809	13.895437	-0.051932	4.815786
252.774876	8000.528729	13.900442	-0.051904	4.815774
252.940827	8000.487641	13.905447	-0.051934	4.815762
252.937514	8000.558044	13.910451	-0.051934	4.815782
253.042325	8000.604579	13.915456	-0.051953	4.815795
252.912552	8000.592853	13.920461	-0.051929	4.815793
252.806482	8000.455530	13.925466	-0.051909	4.815753
253.076229	8000.586953	13.930471	-0.051959	4.815790
253.007056	8000.589024	13.935475	-0.051946	4.815791
253.057262	8000.600507	13.940480	-0.051955	4.815794
252.957488	8000.550832	13.945485	-0.051937	4.815780
252.740351	8000.551567	13.950490	-0.051896	4.815781
253.046583	8000.573615	13.955495	-0.051953	4.815786
253.000904	8000.517346	13.960499	-0.051944	4.815770
252.771687	8000.504005	13.965504	-0.051902	4.815767
252.860725	8000.588720	13.970509	-0.051918	4.815792
252.977591	8000.567120	13.975514	-0.051940	4.815785
252.997928	8000.526871	13.980519	-0.051943	4.815773
252.961550	8000.500647	13.985523	-0.051937	4.815765
252.898388	8000.581822	13.990528	-0.051925	4.815789
252.947370	8000.576203	13.995533	-0.051934	4.815788
252.774746	8000.576593	14.000538	-0.051902	4.815789
253.037857	8000.530678	14.005543	-0.051950	4.815774
253.060710	8000.557732	14.010547	-0.051955	4.815782
252.896375	8000.570001	14.015552	-0.051924	4.815786
252.899143	8000.557225	14.020557	-0.051924	4.815782
252.921089	8000.483904	14.025562	-0.051928	4.815761
252.895011	8000.583831	14.030567	-0.051923	4.815790
252.900929	8000.568971	14.035571	-0.051924	4.815786
253.025355	8000.603013	14.040576	-0.051947	4.815795
252.822473	8000.475861	14.045581	-0.051909	4.815759
252.845102	8000.619286	14.050586	-0.051914	4.815801
252.969070	8000.529471	14.055591	-0.051937	4.815774
252.994850	8000.551234	14.060595	-0.051941	4.815780
253.142534	8000.474617	14.065600	-0.051969	4.815757
253.095909	8000.583820	14.070605	-0.051960	4.815789
253.185373	8000.606618	14.075610	-0.051976	4.815795
252.951223	8000.513122	14.080615	-0.051933	4.815769
252.936896	8000.601496	14.085619	-0.051930	4.815795
253.153335	8000.499305	14.090624	-0.051970	4.815764
253.067311	8000.585447	14.095629	-0.051954	4.815790
252.864710	8000.550117	14.100634	-0.051916	4.815780
253.108533	8000.595708	14.105639	-0.051962	4.815793
253.141591	8000.491605	14.110643	-0.051968	4.815762
253.047386	8000.617117	14.115648	-0.051950	4.815799
253.011662	8000.523642	14.120653	-0.051943	4.815772
252.915106	8000.482561	14.125658	-0.051925	4.815760
252.946068	8000.505476	14.130663	-0.051931	4.815767
252.975815	8000.516627	14.135667	-0.051936	4.815770
252.945839	8000.405095	14.140672	-0.051930	4.815738
253.019357	8000.507707	14.145677	-0.051944	4.815767
252.827340	8000.577180	14.150682	-0.051908	4.815789
253.002045	8000.602430	14.155687	-0.051941	4.815795
253.099674	8000.492970	14.160691	-0.051959	4.815763
253.142358	8000.535293	14.165696	-0.051967	4.815775
253.055550	8000.388673	14.170701	-0.051950	4.815732
253.065714	8000.590617	14.175706	-0.051952	4.815791
253.062586	8000.525430	14.180711	-0.051951	4.815772
252.920635	8000.594648	14.185715	-0.051925	4.815793
253.101712	8000.445973	14.190720	-0.051958	4.815749
252.890292	8000.595205	14.195725	-0.051919	4.815793
252.872172	8000.591699	14.200730	-0.051916	4.815793
252.940248	8000.437986	14.205735	-0.051928	4.815747
252.787118	8000.587097	14.210739	-0.051900	4.815792
252.720786	8000.615905	14.215744	-0.051887	4.815800
252.813460	8000.477538	14.220749	-0.051904	4.815759
252.764040	8000.577086	14.225754	-0.051895	4.815789
252.861550	8000.576526	14.230759	-0.051913	4.815788
252.842312	8000.526025	14.235763	-0.051909	4.815774
252.976749	8000.544214	14.240768	-0.051934	4.815778
252.872049	8000.524354	14.245773	-0.051915	4.815773
252.804661	8000.510439	14.250778	-0.051902	4.815769
252.944438	8000.507362	14.255783	-0.051928	4.815768
253.125236	8000.595703	14.260787	-0.051961	4.815793
253.053226	8000.517653	14.265792	-0.051948	4.815770
252.791885	7999.450051	14.270797	-0.051898	4.815459

252.912946	7996.223938	14.275802	-0.051919	4.814515
253.138606	7990.702657	14.280807	-0.051957	4.812899
253.020041	7983.977763	14.285811	-0.051931	4.810931
252.818222	7976.645604	14.290816	-0.051888	4.808786
252.961864	7969.048281	14.295821	-0.051910	4.806560
253.004611	7961.205786	14.300826	-0.051913	4.804261
252.946565	7953.358062	14.305831	-0.051897	4.801961
252.773187	7945.362376	14.310835	-0.051859	4.799616
252.869850	7937.422504	14.315840	-0.051872	4.797285
252.846887	7929.476222	14.320845	-0.051862	4.794952
252.576185	7921.367713	14.325850	-0.051806	4.792571
252.551870	7913.411256	14.330855	-0.051796	4.790233
252.491510	7905.371160	14.335859	-0.051780	4.787869
252.368509	7897.413776	14.340864	-0.051752	4.785528
252.449818	7889.406907	14.345869	-0.051762	4.783171
252.239588	7881.371453	14.350874	-0.051717	4.780806
252.510875	7873.427973	14.355879	-0.051762	4.778464
252.425670	7865.383079	14.360883	-0.051741	4.776093
252.197746	7857.410247	14.365888	-0.051693	4.773743
251.998016	7849.383614	14.370893	-0.051651	4.771375
252.079982	7841.361369	14.375898	-0.051661	4.769006
252.130358	7833.419842	14.380903	-0.051665	4.766660
251.965685	7825.362396	14.385907	-0.051629	4.764280
252.021987	7817.411946	14.390912	-0.051634	4.761929
252.041482	7809.348917	14.395917	-0.051632	4.759544
251.896943	7801.414611	14.400922	-0.051600	4.757196
252.034879	7793.389427	14.405927	-0.051620	4.754819
251.881055	7785.346029	14.410931	-0.051586	4.752437
251.904302	7777.281272	14.415936	-0.051585	4.750046
251.825070	7769.356309	14.420941	-0.051565	4.747696
251.895535	7761.266454	14.425946	-0.051573	4.745296
251.805796	7753.356724	14.430951	-0.051551	4.742948
251.754345	7745.346248	14.435955	-0.051536	4.740569
251.563696	7737.322691	14.440960	-0.051495	4.738185
251.479053	7729.364121	14.445965	-0.051474	4.735820
251.348844	7721.317846	14.450970	-0.051445	4.733427
251.358622	7713.313706	14.455975	-0.051441	4.731045
251.354200	7705.287268	14.460979	-0.051435	4.728655
251.406258	7697.321978	14.465984	-0.051440	4.726282
251.162388	7689.294221	14.470989	-0.051389	4.723890
251.091215	7681.342229	14.475994	-0.051370	4.721518
251.271045	7673.308482	14.480999	-0.051398	4.719121
251.013133	7665.363029	14.486003	-0.051345	4.716750
251.230387	7657.340799	14.491008	-0.051380	4.714353
251.034504	7649.307886	14.496013	-0.051338	4.711953
251.105313	7641.269677	14.501018	-0.051346	4.709550
250.990891	7633.331235	14.506023	-0.051320	4.707176
250.899580	7625.271863	14.511027	-0.051297	4.704764
250.885266	7617.317274	14.516032	-0.051289	4.702382
250.865705	7609.357317	14.521037	-0.051280	4.699998
250.829985	7601.298218	14.526042	-0.051268	4.697582
250.815939	7593.312117	14.531047	-0.051261	4.695187
250.521915	7585.339815	14.536051	-0.051201	4.692796
250.422100	7577.277208	14.541056	-0.051177	4.690376
250.564657	7569.286724	14.546061	-0.051198	4.687976
250.598565	7561.274749	14.551066	-0.051199	4.685568
250.522657	7553.305742	14.556071	-0.051179	4.683172
250.556518	7545.277094	14.561075	-0.051180	4.680757
250.638435	7537.321272	14.566080	-0.051190	4.678362
250.696021	7529.355909	14.571085	-0.051196	4.675964
250.305028	7521.198810	14.576090	-0.051118	4.673507
250.423210	7513.173710	14.581095	-0.051134	4.671087
250.343326	7505.225367	14.586099	-0.051114	4.668690
250.201688	7497.233315	14.591104	-0.051082	4.666279
250.232324	7489.213040	14.596109	-0.051083	4.663857
250.148812	7481.253339	14.601114	-0.051062	4.661453
249.949627	7473.288089	14.606119	-0.051019	4.659046
250.004142	7465.279359	14.611123	-0.051024	4.656624
250.043867	7457.244820	14.616128	-0.051026	4.654194
249.800080	7449.238397	14.621133	-0.050976	4.651770
249.815807	7441.181299	14.626138	-0.050973	4.649330
250.002501	7433.275129	14.631143	-0.051003	4.646934
249.849462	7425.186874	14.636147	-0.050969	4.644482
249.684927	7417.239787	14.641152	-0.050933	4.642072
249.716684	7409.221174	14.646157	-0.050934	4.639638
249.673182	7401.289893	14.651162	-0.050920	4.637230
249.553799	7393.227031	14.656167	-0.050893	4.634780
249.492539	7385.181913	14.661171	-0.050876	4.632335
249.724866	7377.149624	14.666176	-0.050914	4.629892
249.374593	7369.215302	14.671181	-0.050843	4.627478
249.286481	7361.162443	14.676186	-0.050822	4.625026
249.716092	7353.209483	14.681191	-0.050896	4.622603
249.542280	7345.195789	14.686195	-0.050859	4.620161
249.457297	7337.199731	14.691200	-0.050837	4.617723
249.435869	7329.196684	14.696205	-0.050828	4.615281
249.167169	7321.167267	14.701210	-0.050773	4.612830
249.155469	7313.154391	14.706215	-0.050765	4.610383
248.952754	7305.149981	14.711219	-0.050722	4.607936
248.962868	7297.139533	14.716224	-0.050719	4.605487
248.891121	7289.179344	14.721229	-0.050700	4.603052
248.878045	7281.147875	14.726234	-0.050692	4.600594
248.861374	7273.237923	14.731239	-0.050684	4.598171
248.839728	7265.192608	14.736243	-0.050675	4.595706
248.730252	7257.128365	14.741248	-0.050649	4.593234
248.932213	7249.111662	14.746253	-0.050681	4.590775
248.838428	7241.107955	14.751258	-0.050658	4.588319
248.839323	7233.141900	14.756263	-0.050653	4.585873
248.555308	7225.139173	14.761267	-0.050595	4.583414
248.737928	7217.146695	14.766272	-0.050624	4.580957
248.716286	7209.160053	14.771277	-0.050614	4.578501
248.423120	7201.152188	14.776282	-0.050554	4.576036
248.483532	7193.157729	14.781287	-0.050560	4.573575
248.516113	7185.105852	14.786291	-0.050561	4.571094
248.341782	7177.105687	14.791296	-0.050523	4.568628
248.168035	7169.133192	14.796301	-0.050486	4.566169
248.162839	7161.125943	14.801306	-0.050479	4.563699
248.238236	7153.176278	14.806311	-0.050488	4.561244
248.119622	7145.163028	14.811315	-0.050461	4.558769
248.323396	7137.174901	14.816320	-0.050493	4.556300
248.319613	7129.108265	14.821325	-0.050487	4.553806
248.130072	7121.067174	14.826330	-0.050447	4.551318
248.045024	7113.082441	14.831335	-0.050426	4.548846
247.999004	7105.106916	14.836339	-0.050412	4.546375
247.804660	7097.113425	14.841344	-0.050370	4.543898
247.872006	7089.181234	14.846349	-0.050377	4.541438
248.026752	7081.113967	14.851354	-0.050401	4.538936
247.779494	7073.193352	14.856359	-0.050350	4.536476
247.375379	7065.095251	14.861363	-0.050269	4.533960
247.669018	7057.090609	14.866368	-0.050318	4.531473
247.746675	7049.064621	14.871373	-0.050327	4.528978
247.380582	7041.106329	14.876378	-0.050254	4.526501
247.552992	7033.089520	14.881383	-0.050281	4.524006
247.612772	7025.178118	14.886387	-0.050287	4.521542
247.364675	7017.168176	14.891392	-0.050235	4.519046
247.241807	7009.157791	14.896397	-0.050207	4.516548
247.252151	7001.081803	14.901402	-0.050203	4.514028
247.465857	6993.017671	14.906407	-0.050238	4.511512
247.235009	6985.019633	14.911411	-0.050190	4.509013
247.151880	6977.047839	14.916416	-0.050169	4.506522
247.346421	6969.055111	14.921421	-0.050200	4.504023
246.969642	6961.088808	14.926426	-0.050124	4.501530
246.995230	6953.088508	14.931431	-0.050124	4.499026
246.971399	6945.106076	14.936435	-0.050114	4.496526
247.040375	6937.052519	14.941440	-0.050121	4.494002
247.002150	6929.088124	14.946445	-0.050109	4.491505
246.934838	6921.035945	14.951450	-0.050091	4.488978
246.999957	6913.096374	14.956455	-0.050098	4.486487
246.607076	6905.044665	14.961459	-0.050020	4.483956
246.702825	6897.073989	14.966464	-0.050032	4.481452
246.693825	6889.068159	14.971469	-0.050025	4.478935
246.482896	6881.074986	14.976474	-0.049980	4.476419
246.447570	6873.083466	14.981479	-0.049969	4.473904
246.655030	6865.022382	14.986483	-0.050002	4.471365
246.667506	6857.003688	14.991488	-0.049999	4.468838
246.647679	6849.052269	14.996493	-0.049990	4.466331
246.443444	6840.972970	15.001498	-0.049946	4.463781
246.566744	6833.072408	15.006503	-0.049964	4.461288
246.394779	6825.047415	15.011507	-0.049927	4.458753
246.227099	6817.055650	15.016512	-0.049890	4.456226
246.270904	6809.067800	15.021517	-0.049893	4.453700
246.095506	6800.990605	15.026522	-0.049855	4.451144
246.264513	6793.032947	15.031527	-0.049881	4.448626
246.089324	6785.008404	15.036531	-0.049843	4.446083
245.996668	6777.018937	15.041536	-0.049821	4.443551
246.075049	6769.055370	15.046541	-0.049830	4.441025
246.111277	6761.009345	15.051546	-0.049832	4.438473
246.088273	6753.074943	15.056551	-0.049822	4.435953
245.814647	6745.008112	15.061555	-0.049766	4.433390
245.762656	6736.949759	15.066560	-0.049751	4.430828
245.942518	6728.959457	15.071565	-0.049779	4.428288
245.924933	6720.936374	15.076570	-0.049770	4.425735
245.653395	6712.999165	15.081575	-0.049714	4.423206
245.654230	6704.960606	15.086579	-0.049709	4.420645
245.656813	6697.005994	15.091584	-0.049704	4.418109
245.531935	6689.001177	15.096589	-0.049676	4.415556
245.578134	6680.958266	15.101594	-0.049679	4.412989
245.478941	6672.957522	15.106599	-0.049655	4.410434
245.443381	6664.987789	15.111603	-0.049643	4.407887
245.367046	6656.938414	15.116608	-0.049624	4.405313
245.200605	6649.004544	15.121613	-0.049588	4.402774
245.198748	6640.971168	15.126618	-0.049582	4.400203
245.134450	6633.045877	15.131623	-0.049565	4.397665
245.061276	6625.014313	15.136627	-0.049546	4.395090
245.065283	6617.012443	15.141632	-0.049541	4.392525
245.017359	6608.959736	15.146637	-0.049527	4.389941
244.852028	6600.978037	15.151642	-0.049491	4.387378
245.065941	6592.967107	15.156647	-0.049525	4.384806
244.899273	6585.000678	15.161651	-0.049489	4.382245
244.920352	6576.963740	15.166656	-0.049487	4.379660
244.942265	6569.055688	15.171661	-0.049486	4.377116
244.603647	6560.957304	15.176666	-0.049418	4.374507
244.519929	6552.988927	15.181671	-0.049397	4.371939
244.391315	6544.936077	15.186675	-0.049368	4.369342
244.562134	6536.999417	15.191680	-0.049394	4.366784
244.598395	6528.996457	15.196685	-0.049396	4.364201
244.449569	6521.022148	15.201690	-0.049363	4.361625
244.436943	6513.004525	15.206695	-0.049355	4.359034
244.517566	6505.021677	15.211699	-0.049365	4.356454
244.516098	6496.937132	15.216704	-0.049359	4.353839
244.415742	6488.849824	15.221709	-0.049335	4.351220
244.464190	6480.905067	15.226714	-0.049339	4.348648
244.451326	6472.977829	15.231719	-0.049331	4.346078
244.219654	6464.960734	15.236723	-0.049283	4.343477
244.071738	6456.958316	15.241728	-0.049250	4.340880
244.175714	6448.964999	15.246733	-0.049264	4.338285
244.099540	6440.974540	15.251738	-0.049244	4.335689
244.028382	6432.965754	15.256743	-0.049226	4.333085
243.988048	6424.960183	15.261747	-0.049213	4.330481
243.835627	6416.942748	15.266752	-0.049179	4.327871
243.978397	6408.936100	15.271757	-0.049200	4.325265
243.937415	6400.950812	15.276762	-0.049188	4.322663
243.849430	6392.966636	15.281767	-0.049166	4.320059
243.645503	6384.964138	15.286771	-0.049123	4.317447
243.757026	6376.947824	15.291776	-0.049138	4.314831
243.910934	6368.940128	15.296781	-0.049161	4.312216
243.396641	6360.898470	15.301786	-0.049060	4.309584
243.778348	6352.934284	15.306791	-0.049126	4.306983
243.717780	6344.901374	15.311795	-0.049109	4.304354
243.538878	6336.942019	15.316800	-0.049071	4.301746
243.517589	6328.929452	15.321805	-0.049061	4.299121
243.396431	6320.939467	15.326810	-0.049034	4.296500
243.415582	6312.959523	15.331815	-0.049032	4.293883
243.257901	6304.888039	15.336819	-0.048997	4.291232
243.235599	6296.902805	15.341824	-0.048988	4.288610
243.227961	6288.934450	15.346829	-0.048981	4.285991
243.154431	6280.899566	15.351834	-0.048962	4.283348
243.104566	6272.952544	15.356839	-0.048947	4.280733
242.865633	6264.929016	15.361843	-0.048898	4.278089
242.995098	6256.951197	15.366848	-0.048916	4.275462
242.665882	6248.905974	15.371853	-0.048850	4.272807
242.742179	6240.834389	15.376858	-0.048859	4.270145
242.842360	6232.914693	15.381863	-0.048872	4.267532
242.637710	6224.849205	15.386867	-0.048828	4.264866
242.744572	6216.914566	15.391872	-0.048843	4.262245
242.964617	6208.880714	15.396877	-0.048879	4.259591
242.689932	6200.959629	15.401882	-0.048822	4.256967
242.594934	6192.913228	15.406887	-0.048799	4.254302
242.496166	6184.933255	15.411891	-0.048776	4.251658
242.382619	6176.864559	15.416896	-0.048749	4.248982
242.197773	6168.919673	15.421901	-0.048709	4.246345
242.203722	6160.864394	15.426906	-0.048705	4.243671
242.220475	6152.970818	15.431911	-0.048703	4.241049
242.294157	6144.919903	15.436915	-0.048711	4.238374
242.086937	6136.937531	15.441920	-0.048668	4.235718
242.074141	6128.916154	15.446925	-0.048660	4.233049
241.965339	6120.913906	15.451930	-0.048634	4.230383
242.080787	6112.913896	15.456935	-0.048650	4.227719
242.086556	6104.909972	15.461939	-0.048646	4.225050
242.073721	6096.929441	15.466944	-0.048638	4.222388
241.908588	6088.943570	15.471949	-0.048602	4.219720
241.875477	6080.955097	15.476954	-0.048591	4.217052
242.096883	6072.951821	15.481959	-0.048627	4.214379
241.725735	6064.948349	15.486963	-0.048552	4.211698
241.664201	6056.907021	15.491968	-0.048536	4.209007
241.790623	6048.967562	15.496973	-0.048554	4.206349
241.748491	6040.921910	15.501978	-0.048541	4.203653
241.830343	6032.977150	15.506983	-0.048551	4.200990
241.617526	6024.976941	15.511987	-0.048506	4.198303
241.456687	6016.931958	15.516992	-0.048470	4.195600
241.246361	6008.886383	15.521997	-0.048426	4.192895
241.091204	6000.782118	15.527002	-0.048392	4.190169
241.431557	5992.859217	15.532007	-0.048450	4.187508
241.124940	5984.862144	15.537011	-0.048387	4.184812
241.130562	5976.885150	15.542016	-0.048383	4.182126
241.182155	5968.933072	15.547021	-0.048387	4.179446
240.961166	5960.924780	15.552026	-0.048341	4.176743
241.101951	5952.893994	15.557031	-0.048362	4.174034
241.060128	5944.894825	15.562035	-0.048349	4.171332
241.016647	5936.882447	15.567040	-0.048335	4.168624
241.016049	5928.908921	15.572045	-0.048330	4.165928
240.917830	5920.906997	15.577050	-0.048306	4.163219
240.904338	5912.904659	15.582055	-0.048298	4.160510
240.753412	5904.946370	15.587059	-0.048265	4.157812
240.602769	5896.922421	15.592064	-0.048232	4.155090
240.832252	5888.886865	15.597069	-0.048269	4.152366
240.562162	5880.835399	15.602074	-0.048213	4.149630
240.613496	5872.919519	15.607079	-0.048218	4.146942
240.484019	5864.873771	15.612083	-0.048188	4.144205
240.548577	5856.907227	15.617088	-0.048195	4.141496
240.645047	5848.895217	15.622093	-0.048208	4.138770
240.404363	5840.900602	15.627098	-0.048158	4.136044
240.341413	5832.851812	15.632103	-0.048140	4.133301
240.463764	5824.848324	15.637107	-0.048158	4.130573
240.397013	5816.875295	15.642112	-0.048140	4.127851
240.223974	5808.887710	15.647117	-0.048103	4.125121
240.121825	5800.908349	15.652122	-0.048078	4.122393
240.312816	5792.896947	15.657127	-0.048109	4.119656
240.236708	5784.940005	15.662131	-0.048089	4.116932
239.875725	5776.914305	15.667136	-0.048017	4.114180
239.789879	5768.872810	15.672141	-0.047995	4.111423
239.806900	5760.812819	15.677146	-0.047993	4.108660
239.804462	5752.870880	15.682151	-0.047987	4.105935
239.677354	5744.881734	15.687155	-0.047958	4.103190
239.509763	5736.916814	15.692160	-0.047922	4.100452
239.566560	5728.915010	15.697165	-0.047927	4.097702
239.512338	5720.880246	15.702170	-0.047912	4.094937
239.283260	5712.907643	15.707175	-0.047864	4.092189
239.514809	5704.880708	15.712179	-0.047902	4.089427
239.556070	5696.923666	15.717184	-0.047904	4.086685
239.605677	5688.887482	15.722189	-0.047908	4.083913
239.335719	5680.955386	15.727194	-0.047852	4.081172
239.424828	5672.958322	15.732199	-0.047864	4.078410
239.256749	5664.983327	15.737203	-0.047827	4.075652
239.336539	5656.909034	15.742208	-0.047836	4.072860
239.215006	5648.898934	15.747213	-0.047808	4.070086
239.091515	5640.924169	15.752218	-0.047780	4.067322
239.217303	5632.926638	15.757223	-0.047798	4.064552
239.111016	5624.946789	15.762227	-0.047773	4.061782
238.987338	5616.905713	15.767232	-0.047745	4.058990
239.042089	5608.964341	15.772237	-0.047750	4.056232
238.863126	5600.940252	15.777242	-0.047711	4.053441
238.932175	5592.925705	15.782247	-0.047719	4.050655
238.892322	5584.924838	15.787251	-0.047706	4.047869
238.688544	5576.924805	15.792256	-0.047663	4.045080
238.766532	5568.983747	15.797261	-0.047672	4.042314
238.650722	5560.940061	15.802266	-0.047645	4.039507
238.613780	5552.983585	15.807271	-0.047633	4.036730
238.501869	5544.918779	15.812275	-0.047607	4.033911
238.478031	5536.796012	15.817280	-0.047597	4.031072
238.588647	5528.866771	15.822285	-0.047612	4.028301
238.149481	5520.865354	15.827290	-0.047525	4.025494
238.199726	5512.923936	15.832295	-0.047529	4.022713
238.136510	5504.928888	15.837299	-0.047512	4.019910
238.083763	5496.944326	15.842304	-0.047497	4.017109
238.012356	5488.924398	15.847309	-0.047478	4.014294
238.025039	5480.876157	15.852314	-0.047475	4.011467
238.039327	5472.901009	15.857319	-0.047473	4.008665
237.899410	5464.903790	15.862323	-0.047441	4.005850
237.885990	5456.910959	15.867328	-0.047433	4.003037
237.918311	5448.933197	15.872333	-0.047434	4.000227
237.691036	5440.947219	15.877338	-0.047387	3.997409
237.976150	5432.923103	15.882343	-0.047434	3.994584
237.947104	5424.896043	15.887347	-0.047424	3.991750
237.860243	5416.867659	15.892352	-0.047402	3.988913
237.809059	5408.885755	15.897357	-0.047387	3.986091
237.633073	5400.924183	15.902362	-0.047349	3.983272
237.599221	5392.937858	15.907367	-0.047338	3.980445
237.529997	5384.967704	15.912371	-0.047319	3.977621
237.573182	5376.917811	15.917376	-0.047322	3.974768
237.520119	5368.948642	15.922381	-0.047307	3.971941
237.255086	5360.896804	15.927386	-0.047252	3.969078
237.212737	5352.972906	15.932391	-0.047239	3.966263
237.262515	5344.985266	15.937395	-0.047243	3.963424
237.437052	5336.959594	15.942400	-0.047270	3.960572
237.325157	5329.017503	15.947405	-0.047244	3.957743
237.339439	5320.976892	15.952410	-0.047241	3.954879
236.959970	5312.963075	15.957415	-0.047165	3.952016
236.969529	5304.931798	15.962419	-0.047162	3.949150
237.117670	5296.924885	15.967424	-0.047184	3.946294
237.231199	5288.919309	15.972429	-0.047200	3.943436
236.919728	5280.961517	15.977434	-0.047137	3.940586
237.070025	5273.004956	15.982439	-0.047159	3.937741
236.986835	5264.990794	15.987443	-0.047139	3.934870
236.714422	5256.981563	15.992448	-0.047082	3.931996
236.762125	5248.980470	15.997453	-0.047086	3.929128
236.611855	5240.999562	16.002458	-0.047053	3.926261
236.764946	5232.985696	16.007463	-0.047076	3.923386
236.477176	5225.015733	16.012467	-0.047017	3.920516
236.355154	5216.995532	16.017472	-0.046989	3.917630
236.391338	5209.007001	16.022477	-0.046990	3.914755
236.423028	5200.955240	16.027482	-0.046991	3.911856
236.208574	5192.981048	16.032487	-0.046946	3.908978
236.473694	5184.981015	16.037491	-0.046990	3.906097
236.211136	5176.977955	16.042496	-0.046936	3.903203
236.218301	5168.994492	16.047501	-0.046932	3.900320
236.188107	5161.011128	16.052506	-0.046921	3.897433
236.229675	5153.018704	16.057511	-0.046923	3.894542
236.198248	5144.983480	16.062515	-0.046912	3.891633
236.120463	5136.981725	16.067520	-0.046892	3.888732
236.125303	5128.996213	16.072525	-0.046888	3.885837
235.860497	5120.984626	16.077530	-0.046833	3.882924
235.759293	5112.997036	16.082535	-0.046809	3.880022
235.695552	5105.032350	16.087539	-0.046792	3.877126
235.680115	5096.956906	16.092544	-0.046784	3.874189
235.629626	5088.746305	16.097549	-0.046769	3.871200
235.677113	5080.822059	16.102554	-0.046772	3.868314
235.732025	5072.857074	16.107559	-0.046777	3.865412
235.565063	5064.952136	16.112563	-0.046741	3.862525
235.379728	5056.937076	16.117568	-0.046701	3.859596
235.417693	5049.023498	16.122573	-0.046703	3.856705
235.206571	5040.973431	16.127578	-0.046658	3.853758
235.317031	5032.998746	16.132583	-0.046673	3.850842
235.269903	5024.973224	16.137587	-0.046659	3.847902
235.356600	5016.954038	16.142592	-0.046670	3.844965
235.216932	5009.035354	16.147597	-0.046639	3.842059
235.091957	5001.020713	16.152602	-0.046610	3.839115
235.083821	4993.052405	16.157607	-0.046603	3.836188
235.116829	4985.020782	16.162611	-0.046604	3.833236
234.991319	4976.986546	16.167616	-0.046576	3.830278
234.958692	4969.032110	16.172621	-0.046564	3.827349
234.795907	4961.003997	16.177626	-0.046529	3.824388
234.828793	4953.089422	16.182631	-0.046529	3.821470
234.671312	4945.095452	16.187635	-0.046495	3.818517
234.691010	4937.049312	16.192640	-0.046493	3.815546
234.627737	4929.100390	16.197645	-0.046476	3.812607
234.407662	4921.033454	16.202650	-0.046430	3.809619
234.621056	4913.080813	16.207655	-0.046464	3.806680
234.636431	4905.034641	16.212659	-0.046462	3.803699
234.516507	4897.103757	16.217664	-0.046434	3.800757
234.525792	4889.120973	16.222669	-0.046431	3.797795
234.342455	4881.111286	16.227674	-0.046391	3.794817
234.220604	4873.072405	16.232679	-0.046363	3.791827
234.177419	4865.072995	16.237683	-0.046350	3.788851
234.341124	4857.020560	16.242688	-0.046375	3.785858
234.213654	4849.105016	16.247693	-0.046346	3.782907
234.102795	4841.061599	16.252698	-0.046320	3.779906
233.880971	4833.135055	16.257703	-0.046273	3.776944
233.893095	4825.074440	16.262707	-0.046270	3.773934
233.936507	4817.056773	16.267712	-0.046273	3.770939
233.837137	4809.099235	16.272717	-0.046249	3.767961
233.894947	4801.062540	16.277722	-0.046255	3.764955
233.940376	4793.127156	16.282727	-0.046258	3.761984
233.915400	4785.112451	16.287731	-0.046248	3.758979
233.749337	4777.130355	16.292736	-0.046212	3.755980
233.824948	4769.119789	16.297741	-0.046220	3.752974
233.517512	4761.064677	16.302746	-0.046158	3.749940
233.552683	4753.103573	16.307751	-0.046159	3.746947
233.704655	4745.087619	16.312755	-0.046182	3.743934
233.614630	4737.132182	16.317760	-0.046160	3.740935
233.566900	4729.158983	16.322765	-0.046146	3.737929
233.430517	4721.132476	16.327770	-0.046115	3.734897
233.184716	4713.169897	16.332775	-0.046064	3.731885
233.156118	4705.149691	16.337779	-0.046053	3.728853
233.084426	4697.128870	16.342784	-0.046035	3.725818
233.102410	4689.190516	16.347789	-0.046033	3.722814
232.827955	4681.188339	16.352794	-0.045976	3.719776
233.014691	4673.202691	16.357799	-0.046006	3.716753
232.921109	4665.163404	16.362803	-0.045983	3.713700
232.790039	4657.086358	16.367808	-0.045953	3.710629
232.929858	4649.114266	16.372813	-0.045974	3.707603
232.811790	4641.102233	16.377818	-0.045947	3.704552
232.675793	4633.175085	16.382823	-0.045916	3.701531
232.702719	4625.204496	16.387827	-0.045916	3.698495
232.792523	4617.173302	16.392832	-0.045927	3.695435
232.540428	4609.227658	16.397837	-0.045875	3.692396
232.391868	4601.169901	16.402842	-0.045842	3.689315
232.403795	4593.210366	16.407847	-0.045839	3.686273
232.621291	4585.231516	16.412851	-0.045874	3.683225
232.433113	4577.212848	16.417856	-0.045834	3.680150
232.578939	4569.253579	16.422861	-0.045855	3.677104
232.416401	4561.214917	16.427866	-0.045820	3.674016
232.149681	4553.218544	16.432871	-0.045765	3.670940
232.092714	4545.219739	16.437875	-0.045749	3.667866
232.162626	4537.197998	16.442880	-0.045757	3.664783
232.277428	4529.248057	16.447885	-0.045773	3.661726
232.120910	4521.233211	16.452890	-0.045738	3.658635
231.933684	4513.294499	16.457895	-0.045698	3.655570
232.158780	4505.232439	16.462899	-0.045735	3.652466
231.937674	4497.205296	16.467904	-0.045688	3.649360
231.874217	4489.279229	16.472909	-0.045671	3.646295
231.961175	4481.252676	16.477914	-0.045682	3.643193
232.042466	4473.273625	16.482919	-0.045692	3.640106
231.658193	4465.315055	16.487923	-0.045615	3.637012
231.696874	4457.256783	16.492928	-0.045617	3.633888
231.621464	4449.235090	16.497933	-0.045597	3.630773
231.486689	4441.228488	16.502938	-0.045567	3.627659
231.545087	4433.203249	16.507943	-0.045573	3.624541
231.619166	4425.278427	16.512947	-0.045581	3.621459
231.589446	4417.279498	16.517952	-0.045570	3.618343
231.659576	4409.300437	16.522957	-0.045578	3.615234
231.378798	4401.278686	16.527962	-0.045520	3.612097
231.407821	4393.285183	16.532967	-0.045520	3.608977
231.207413	4385.347670	16.537971	-0.045478	3.605869
231.120080	4377.326842	16.542976	-0.045456	3.602729
231.307826	4369.344364	16.547981	-0.045486	3.599609
231.108773	4361.401288	16.552986	-0.045444	3.596492
230.975171	4353.388865	16.557991	-0.045413	3.593345
231.024077	4345.358422	16.562995	-0.045417	3.590195
230.970381	4337.345618	16.568000	-0.045402	3.587045
231.072302	4329.370647	16.573005	-0.045416	3.583912
230.996880	4321.382214	16.578010	-0.045396	3.580766
230.974993	4313.405650	16.583015	-0.045387	3.577624
230.785249	4305.408024	16.588019	-0.045346	3.574465
230.809951	4297.391545	16.593024	-0.045345	3.571303
230.619822	4289.413767	16.598029	-0.045305	3.568146
230.596937	4281.377914	16.603034	-0.045295	3.564969
230.526795	4273.445804	16.608039	-0.045277	3.561829
230.697397	4265.428804	16.613043	-0.045303	3.558659
230.502118	4257.440562	16.618048	-0.045262	3.555487
230.373898	4249.364872	16.623053	-0.045232	3.552279
230.425023	4241.321647	16.628058	-0.045237	3.549087
230.435265	4233.364868	16.633063	-0.045233	3.545925
230.342961	4225.424459	16.638067	-0.045211	3.542764
230.248335	4217.398873	16.643072	-0.045188	3.539566
230.327984	4209.447306	16.648077	-0.045197	3.536399
230.166791	4201.420914	16.653082	-0.045162	3.533193
229.945823	4193.436909	16.658087	-0.045115	3.529999
229.906300	4185.454242	16.663091	-0.045103	3.526808
229.861954	4177.434718	16.668096	-0.045089	3.523599
229.764810	4169.514649	16.673101	-0.045066	3.520425
229.669407	4161.494160	16.678106	-0.045043	3.517209
229.683331	4153.488217	16.683111	-0.045040	3.513999
229.687952	4145.475536	16.688115	-0.045036	3.510782
229.609344	4137.447117	16.693120	-0.045016	3.507554
229.528399	4129.479852	16.698125	-0.044995	3.504347
229.551500	4121.524249	16.703130	-0.044994	3.501146
229.513155	4113.534228	16.708135	-0.044982	3.497926
229.651517	4105.514589	16.713139	-0.045002	3.494696
229.548621	4097.538953	16.718144	-0.044978	3.491473
229.501341	4089.571781	16.723149	-0.044964	3.488253
229.495454	4081.530029	16.728154	-0.044957	3.485001
229.391587	4073.592170	16.733159	-0.044933	3.481784
229.146449	4065.627412	16.738163	-0.044882	3.478550
228.847369	4057.617507	16.743168	-0.044821	3.475292
229.040463	4049.589266	16.748173	-0.044851	3.472039
229.183019	4041.516415	16.753178	-0.044872	3.468764
228.978609	4033.577020	16.758183	-0.044829	3.465529
228.966062	4025.619066	16.763187	-0.044822	3.462289
228.906625	4017.585017	16.768192	-0.044805	3.459014
228.751507	4009.634397	16.773197	-0.044771	3.455766
228.789478	4001.591690	16.778202	-0.044773	3.452484
228.680105	3993.618153	16.783207	-0.044747	3.449223
228.629473	3985.642883	16.788211	-0.044732	3.445959
228.532809	3977.675880	16.793216	-0.044709	3.442695
228.725781	3969.652577	16.798221	-0.044740	3.439414
228.432634	3961.684067	16.803226	-0.044680	3.436135
228.402735	3953.646314	16.808231	-0.044669	3.432835
228.422938	3945.657770	16.813235	-0.044667	3.429552
228.348686	3937.649725	16.818240	-0.044648	3.426256
228.525467	3929.686376	16.823245	-0.044676	3.422983
228.247777	3921.695350	16.828250	-0.044619	3.419680
228.482468	3913.713706	16.833255	-0.044657	3.416396
228.304169	3905.702054	16.838259	-0.044619	3.413081
227.974969	3897.704762	16.843264	-0.044552	3.409765
228.130841	3889.742166	16.848269	-0.044576	3.406476
228.070156	3881.720112	16.853274	-0.044559	3.403151
227.915732	3873.788292	16.858279	-0.044525	3.399858
227.844083	3865.807663	16.863283	-0.044506	3.396544
227.722728	3857.746628	16.868288	-0.044478	3.393191
227.703310	3849.708307	16.873293	-0.044470	3.389849
227.621730	3841.690672	16.878298	-0.044449	3.386509
227.682766	3833.749825	16.883303	-0.044455	3.383203
227.665847	3825.806113	16.888307	-0.044447	3.379890
227.512903	3817.810739	16.893312	-0.044413	3.376547
227.623135	3809.818872	16.898317	-0.044428	3.373212
227.399679	3801.796939	16.903322	-0.044381	3.369849
227.484548	3793.798489	16.908327	-0.044392	3.366504
227.353393	3785.842858	16.913331	-0.044362	3.363165
227.409545	3777.838185	16.918336	-0.044367	3.359809
227.439356	3769.896518	16.923341	-0.044367	3.356475
227.311230	3761.846447	16.928346	-0.044338	3.353087
227.282356	3753.844939	16.933351	-0.044327	3.349719
227.161502	3745.865399	16.938355	-0.044300	3.346354
227.247717	3737.849309	16.943360	-0.044310	3.342978
227.135835	3729.903636	16.948365	-0.044284	3.339620
226.869179	3721.918952	16.953370	-0.044229	3.336237
226.826058	3713.916303	16.958375	-0.044216	3.332851
226.812962	3705.890430	16.963379	-0.044208	3.329454
226.632289	3697.913259	16.968384	-0.044169	3.326066
226.770743	3689.934594	16.973389	-0.044190	3.322687
226.578738	3681.954198	16.978394	-0.044149	3.319291
226.550656	3674.010881	16.983399	-0.044138	3.315914
226.671841	3665.973705	16.988403	-0.044155	3.312499
226.563464	3657.932190	16.993408	-0.044130	3.309070
226.513610	3649.974360	16.998413	-0.044115	3.305675
226.324332	3641.993307	17.003418	-0.044075	3.302261
226.300993	3634.012337	17.008423	-0.044065	3.298850
226.266404	3626.049400	17.013427	-0.044053	3.295443
226.311138	3618.035849	17.018432	-0.044056	3.292014
226.384046	3610.026639	17.023437	-0.044065	3.288584
226.063223	3602.061262	17.028442	-0.044000	3.285154
226.040523	3594.099942	17.033447	-0.043990	3.281734
226.176722	3586.099159	17.038451	-0.044010	3.278300
225.998551	3578.103331	17.043456	-0.043972	3.274852
226.145369	3570.100216	17.048461	-0.043994	3.271409
226.039051	3562.084399	17.053466	-0.043969	3.267948
226.177795	3554.082931	17.058471	-0.043989	3.264499
226.021668	3546.165942	17.063475	-0.043955	3.261071
225.895735	3538.125492	17.068480	-0.043926	3.257587
225.845290	3530.149447	17.073485	-0.043911	3.254130
225.686834	3522.127086	17.078490	-0.043876	3.250645
225.710302	3514.149094	17.083495	-0.043875	3.247183
225.632799	3506.193969	17.088499	-0.043856	3.243724
225.355784	3498.204893	17.093504	-0.043799	3.240237
225.434908	3490.230883	17.098509	-0.043808	3.236768
225.130570	3482.233798	17.103514	-0.043746	3.233270
225.171675	3474.186843	17.108519	-0.043749	3.229760
225.130468	3466.213453	17.113523	-0.043736	3.226274
225.176375	3458.194168	17.118528	-0.043739	3.222769
225.325860	3450.218767	17.123533	-0.043761	3.219283
225.241623	3442.263949	17.128538	-0.043740	3.215793
225.137405	3434.250715	17.133543	-0.043716	3.212273
225.193610	3426.253192	17.138547	-0.043721	3.208762
224.867031	3418.289266	17.143552	-0.043655	3.205246
224.799247	3410.345850	17.148557	-0.043637	3.201747
224.722787	3402.339764	17.153562	-0.043617	3.198215
224.780639	3394.343213	17.158567	-0.043623	3.194689
224.786198	3386.347030	17.163571	-0.043618	3.191158
224.671832	3378.340115	17.168576	-0.043592	3.187612
224.618885	3370.360251	17.173581	-0.043577	3.184078
224.611324	3362.396187	17.178586	-0.043570	3.180548
224.587190	3354.417949	17.183591	-0.043560	3.177007
224.458478	3346.422870	17.188595	-0.043531	3.173451
224.327794	3338.407539	17.193600	-0.043501	3.169881
224.369433	3330.432296	17.198605	-0.043504	3.166333
224.473176	3322.438251	17.203610	-0.043518	3.162774
224.311110	3314.462889	17.208615	-0.043482	3.159209
224.393654	3306.500050	17.213619	-0.043492	3.155656
224.240339	3298.460988	17.218624	-0.043458	3.152054
224.211753	3290.467097	17.223629	-0.043448	3.148474
224.037393	3282.490323	17.228634	-0.043410	3.144892
223.979836	3274.525178	17.233639	-0.043394	3.141315
223.961946	3266.555512	17.238643	-0.043385	3.137734
223.844338	3258.535399	17.243648	-0.043358	3.134122
223.741548	3250.563325	17.248653	-0.043334	3.130528
223.470260	3242.581127	17.253658	-0.043278	3.126918
223.850387	3234.563111	17.258663	-0.043343	3.123316
223.847483	3226.597010	17.263667	-0.043338	3.119717
223.464636	3218.668927	17.268672	-0.043261	3.116113
223.734971	3210.638270	17.273677	-0.043306	3.112489
223.493394	3202.625277	17.278682	-0.043256	3.108845
223.514342	3194.656032	17.283687	-0.043254	3.105228
223.581303	3186.680466	17.288691	-0.043261	3.101607
223.351062	3178.703568	17.293696	-0.043213	3.097967
223.372689	3170.719729	17.298701	-0.043212	3.094331
223.423145	3162.691732	17.303706	-0.043216	3.090672
223.335025	3154.720015	17.308711	-0.043194	3.087028
223.424286	3146.746634	17.313715	-0.043206	3.083387
223.240231	3138.755119	17.318720	-0.043166	3.079721
223.326247	3130.807064	17.323725	-0.043177	3.076083
223.041980	3122.767995	17.328730	-0.043119	3.072381
222.932936	3114.718858	17.333735	-0.043093	3.068679
223.078864	3106.726718	17.338739	-0.043115	3.065010
222.729827	3098.802189	17.343744	-0.043044	3.061345
222.751023	3090.848012	17.348749	-0.043043	3.057679
222.631566	3082.836019	17.353754	-0.043016	3.053975
222.643246	3074.850018	17.358759	-0.043012	3.050286
222.415018	3066.907859	17.363763	-0.042965	3.046600
222.205986	3058.915520	17.368768	-0.042920	3.042888
222.531503	3050.908660	17.373773	-0.042976	3.039190
222.403876	3042.963075	17.378778	-0.042947	3.035494
222.242188	3034.950915	17.383783	-0.042911	3.031761
222.266491	3026.958840	17.388787	-0.042910	3.028042
222.128490	3018.956681	17.393792	-0.042879	3.024305
222.275882	3011.006877	17.398797	-0.042902	3.020603
222.265262	3003.007159	17.403802	-0.042894	3.016864
222.110752	2995.017780	17.408807	-0.042860	3.013119
221.820898	2987.043974	17.413811	-0.042801	3.009370
221.756688	2979.071146	17.418816	-0.042784	3.005628
221.832069	2971.096222	17.423821	-0.042792	3.001886
221.752244	2963.119725	17.428826	-0.042772	2.998132
221.553072	2955.147334	17.433831	-0.042730	2.994369
221.611464	2947.120033	17.438835	-0.042735	2.990589
221.676588	2939.104123	17.443840	-0.042742	2.986809
221.476808	2931.166791	17.448845	-0.042700	2.983048
221.419839	2923.168299	17.453850	-0.042684	2.979261
221.574037	2915.182486	17.458855	-0.042707	2.975485
221.478909	2907.207093	17.463859	-0.042684	2.971697
221.417025	2899.205511	17.468864	-0.042667	2.967894
221.631530	2891.212757	17.473869	-0.042702	2.964104
221.549527	2883.256110	17.478874	-0.042681	2.960311
221.053179	2875.326867	17.483879	-0.042584	2.956505
221.162466	2867.309391	17.488883	-0.042599	2.952683
220.852457	2859.319517	17.493888	-0.042536	2.948847
221.014996	2851.349631	17.498893	-0.042561	2.945041
220.816567	2843.389427	17.503898	-0.042519	2.941216
220.822532	2835.385608	17.508903	-0.042514	2.937375
220.721040	2827.416944	17.513907	-0.042490	2.933540
220.631075	2819.380981	17.518912	-0.042468	2.929669
220.789599	2811.416599	17.523917	-0.042492	2.925840
220.741621	2803.443133	17.528922	-0.042478	2.921991
220.575358	2795.484131	17.533927	-0.042442	2.918138
220.621459	2787.506593	17.538931	-0.042445	2.914281
220.539323	2779.411991	17.543936	-0.042424	2.910356
220.601380	2771.456551	17.548941	-0.042431	2.906501
220.324503	2763.502815	17.553946	-0.042374	2.902624
220.416078	2755.519728	17.558951	-0.042386	2.898747
220.425862	2747.555059	17.563955	-0.042382	2.894869
220.325100	2739.549987	17.568960	-0.042358	2.890960
220.361933	2731.570523	17.573965	-0.042360	2.887066
220.298396	2723.622562	17.578970	-0.042342	2.883177
219.979438	2715.678181	17.583975	-0.042278	2.879270
219.976614	2707.722774	17.588979	-0.042272	2.875369
219.885956	2699.690131	17.593984	-0.042250	2.871421
219.973692	2691.696169	17.598989	-0.042261	2.867496
219.798362	2683.726826	17.603994	-0.042223	2.863563
219.732283	2675.763822	17.608999	-0.042205	2.859634
219.822619	2667.782782	17.614003	-0.042217	2.855700
219.554952	2659.783708	17.619008	-0.042162	2.851731
219.570266	2651.818728	17.624013	-0.042159	2.847789
219.684696	2643.810105	17.629018	-0.042175	2.843825
219.653114	2635.863732	17.634023	-0.042164	2.839879
219.520731	2627.922311	17.639027	-0.042134	2.835924
219.427573	2619.885410	17.644032	-0.042111	2.831918
219.460941	2611.904325	17.649037	-0.042112	2.827942
219.125688	2603.955959	17.654042	-0.042045	2.823955
219.100285	2595.981026	17.659047	-0.042035	2.819967
219.175250	2587.994036	17.664051	-0.042043	2.815973
218.960109	2580.014326	17.669056	-0.041998	2.811960
218.927929	2572.029418	17.674061	-0.041987	2.807950
219.067412	2564.018772	17.679066	-0.042007	2.803931
218.888006	2556.072468	17.684071	-0.041969	2.799919
218.949318	2548.135176	17.689075	-0.041975	2.795921
218.669322	2540.129496	17.694080	-0.041917	2.791862
218.718509	2532.146153	17.699085	-0.041921	2.787828
218.628064	2524.149906	17.704090	-0.041899	2.783774
218.478598	2516.186379	17.709095	-0.041866	2.779727
218.647617	2508.225033	17.714099	-0.041892	2.775693
218.476576	2500.227788	17.719104	-0.041855	2.771616
218.321859	2492.256420	17.724109	-0.041821	2.767546
218.536449	2484.284158	17.729114	-0.041855	2.763492
218.316812	2476.320100	17.734119	-0.041809	2.759410
218.313701	2468.386999	17.739123	-0.041803	2.755352
218.160772	2460.297531	17.744128	-0.041769	2.751197
218.293941	2452.313066	17.749133	-0.041789	2.747108
218.109602	2444.357899	17.754138	-0.041749	2.743009
218.165700	2436.379602	17.759143	-0.041754	2.738906
218.222742	2428.431273	17.764147	-0.041760	2.734812
218.125842	2420.430299	17.769152	-0.041736	2.730676
217.900895	2412.494142	17.774157	-0.041689	2.726559
217.867778	2404.526157	17.779162	-0.041678	2.722431
217.711122	2396.565766	17.784167	-0.041643	2.718293
217.780022	2388.590024	17.789171	-0.041651	2.714155
217.816180	2380.571553	17.794176	-0.041652	2.709986
217.931109	2372.603856	17.799181	-0.041668	2.705842
217.828617	2364.643917	17.804186	-0.041644	2.701682
217.483371	2356.717734	17.809191	-0.041574	2.697519
217.547710	2348.727815	17.814195	-0.041581	2.693341
217.501132	2340.705915	17.819200	-0.041567	2.689133
217.421950	2332.774214	17.824205	-0.041547	2.684963
217.122424	2324.831718	17.829210	-0.041486	2.680767
217.190408	2316.848381	17.834215	-0.041493	2.676567
217.014133	2308.853383	17.839219	-0.041455	2.672338
216.936007	2300.866877	17.844224	-0.041435	2.668114
217.170802	2292.844329	17.849229	-0.041474	2.663883
217.028942	2284.915659	17.854234	-0.041442	2.659672
216.888876	2276.945935	17.859239	-0.041411	2.655432
216.963822	2268.964459	17.864243	-0.041419	2.651193
216.866534	2260.984895	17.869248	-0.041396	2.646937
216.778784	2253.049504	17.874253	-0.041374	2.642698
216.634228	2245.086587	17.879258	-0.041342	2.638434
216.689973	2237.104373	17.884263	-0.041347	2.634166
216.713453	2229.111398	17.889267	-0.041346	2.629883
216.649409	2221.132364	17.894272	-0.041329	2.625595
216.458548	2213.187894	17.899277	-0.041288	2.621310
216.704288	2205.189379	17.904282	-0.041329	2.617017
216.490572	2197.247866	17.909287	-0.041284	2.612718
216.374595	2189.278245	17.914291	-0.041257	2.608403
216.291572	2181.306248	17.919296	-0.041236	2.604082
216.052102	2173.372507	17.924301	-0.041186	2.599764
215.969718	2165.423273	17.929306	-0.041166	2.595441
215.955089	2157.255532	17.934311	-0.041157	2.590996
215.951155	2149.288208	17.939315	-0.041151	2.586654
215.777791	2141.340951	17.944320	-0.041114	2.582303
215.941628	2133.400744	17.949325	-0.041139	2.577973
215.968321	2125.440357	17.954330	-0.041139	2.573614
215.539032	2117.498899	17.959335	-0.041053	2.569227
215.641907	2109.546916	17.964339	-0.041067	2.564864
215.652104	2101.572810	17.969344	-0.041064	2.560474
215.464238	2093.644804	17.974349	-0.041024	2.556089
215.438253	2085.663963	17.979354	-0.041014	2.551678
215.382203	2077.672288	17.984359	-0.040998	2.547251
215.475985	2069.709794	17.989363	-0.041010	2.542843
215.228278	2061.782930	17.994368	-0.040959	2.538424
215.200356	2053.808889	17.999373	-0.040948	2.533986
215.124058	2045.823947	18.004378	-0.040929	2.529530
215.102820	2037.860316	18.009383	-0.040919	2.525083
215.268776	2029.905970	18.014387	-0.040945	2.520646
214.958198	2021.973805	18.019392	-0.040882	2.516180
214.838985	2013.978229	18.024397	-0.040854	2.511684
214.772718	2005.983009	18.029402	-0.040837	2.507183
214.719367	1998.006328	18.034407	-0.040821	2.502686
214.881222	1990.048278	18.039411	-0.040846	2.498208
214.735095	1982.088774	18.044416	-0.040814	2.493697
214.790385	1974.101968	18.049421	-0.040819	2.489178
214.777966	1966.171120	18.054426	-0.040811	2.484678
214.495112	1958.229686	18.059431	-0.040753	2.480143
214.502719	1950.291995	18.064435	-0.040749	2.475624
214.552626	1942.263765	18.069440	-0.040753	2.471047
214.450892	1934.338103	18.074445	-0.040729	2.466510
214.189108	1926.394614	18.079450	-0.040675	2.461942
214.326090	1918.406222	18.084455	-0.040695	2.457370
214.268948	1910.464833	18.089459	-0.040679	2.452801
213.947408	1902.483324	18.094464	-0.040614	2.448181
213.860549	1894.548133	18.099469	-0.040593	2.443597
213.924125	1886.585412	18.104474	-0.040599	2.438999
213.799397	1878.619661	18.109479	-0.040571	2.434377
213.784253	1870.584217	18.114483	-0.040563	2.429714
213.646481	1862.617707	18.119488	-0.040532	2.425072
213.770732	1854.666374	18.124493	-0.040550	2.420451
213.653316	1846.741342	18.129498	-0.040522	2.415818
213.542559	1838.773613	18.134503	-0.040497	2.411151
213.601476	1830.805996	18.139507	-0.040502	2.406488
213.429888	1822.860296	18.144512	-0.040465	2.401811
213.627721	1814.900260	18.149517	-0.040497	2.397146
213.637901	1806.942273	18.154522	-0.040493	2.392457
213.403041	1798.982458	18.159527	-0.040444	2.387740
213.204824	1791.058917	18.164531	-0.040402	2.383037
213.228612	1783.078996	18.169536	-0.040401	2.378309
213.101307	1775.138630	18.174541	-0.040372	2.373583
213.069490	1767.166191	18.179546	-0.040361	2.368836
212.811560	1759.222161	18.184551	-0.040308	2.364078
212.962073	1751.267363	18.189555	-0.040330	2.359338
212.928177	1743.319760	18.194560	-0.040319	2.354577
212.539857	1735.357436	18.199565	-0.040241	2.349769
212.663719	1727.371051	18.204570	-0.040259	2.344978
212.724465	1719.415932	18.209575	-0.040265	2.340191
212.775831	1711.472373	18.214579	-0.040269	2.335400
212.655750	1703.492856	18.219584	-0.040242	2.330564
212.523648	1695.564285	18.224589	-0.040212	2.325747
212.297977	1687.640336	18.229594	-0.040164	2.320916
212.318360	1679.682750	18.234599	-0.040163	2.316074
212.425390	1671.703843	18.239603	-0.040177	2.311217
212.100297	1663.764359	18.244608	-0.040112	2.306337
212.228588	1655.800292	18.249613	-0.040130	2.301470
212.165289	1647.858978	18.254618	-0.040113	2.296590
212.053208	1639.898950	18.259623	-0.040087	2.291684
211.983233	1631.945169	18.264627	-0.040069	2.286775
211.975861	1623.998096	18.269632	-0.040062	2.281865
211.978456	1616.070270	18.274637	-0.040057	2.276958
211.814531	1608.083542	18.279642	-0.040021	2.271988
211.808684	1600.063893	18.284647	-0.040015	2.267001
211.852892	1592.133257	18.289651	-0.040018	2.262063
211.775522	1584.203832	18.294656	-0.039998	2.257104
211.716983	1576.261101	18.299661	-0.039982	2.252128
211.585482	1568.322008	18.304666	-0.039952	2.247136
211.704461	1560.357250	18.309671	-0.039969	2.242139
211.556834	1552.470664	18.314675	-0.039937	2.237157
211.479669	1544.490396	18.319680	-0.039917	2.232111
211.482062	1536.541457	18.324685	-0.039912	2.227080
211.193265	1528.625262	18.329690	-0.039853	2.222032
211.123334	1520.688647	18.334695	-0.039835	2.216980
211.388406	1512.694649	18.339699	-0.039879	2.211909
211.298135	1504.742229	18.344704	-0.039857	2.206821
211.146292	1496.832713	18.349709	-0.039823	2.201744
211.057547	1488.908566	18.354714	-0.039801	2.196651
210.969194	1480.928366	18.359719	-0.039780	2.191510
210.977096	1472.973863	18.364723	-0.039776	2.186383
210.781483	1465.047320	18.369728	-0.039734	2.181242
210.690192	1457.135600	18.374733	-0.039712	2.176109
210.714815	1449.156954	18.379738	-0.039711	2.170931
210.735818	1441.201658	18.384743	-0.039710	2.165755
210.643851	1433.288626	18.389747	-0.039687	2.160584
210.371124	1425.384159	18.394752	-0.039631	2.155390
210.225127	1417.440139	18.399757	-0.039599	2.150168
210.198695	1409.474660	18.404762	-0.039589	2.144931
210.169079	1401.531695	18.409767	-0.039578	2.139696
210.018239	1393.631243	18.414771	-0.039544	2.134464
210.047941	1385.642342	18.419776	-0.039545	2.129179
210.082876	1377.707489	18.424781	-0.039546	2.123916
210.194088	1369.776108	18.429786	-0.039561	2.118650
209.932532	1361.846381	18.434791	-0.039507	2.113336
209.816029	1353.862417	18.439795	-0.039480	2.107986
209.598909	1345.939165	18.444800	-0.039435	2.102654
209.662818	1338.012366	18.449805	-0.039441	2.097333
209.655857	1330.071240	18.454810	-0.039435	2.091982
209.752086	1322.109575	18.459815	-0.039447	2.086613
209.637647	1314.220824	18.464819	-0.039421	2.081259
209.393078	1306.321797	18.469824	-0.039370	2.075872
209.324877	1298.369852	18.474829	-0.039352	2.070452
209.270510	1290.418012	18.479834	-0.039337	2.065019
209.161442	1282.506734	18.484839	-0.039311	2.059594
209.167031	1274.591620	18.489843	-0.039307	2.054164
209.188258	1266.624871	18.494848	-0.039306	2.048685
209.024488	1258.713560	18.499853	-0.039270	2.043211
208.884758	1250.816414	18.504858	-0.039239	2.037734
208.881551	1242.851032	18.509863	-0.039233	2.032210
208.881454	1234.913778	18.514867	-0.039227	2.026690
208.795716	1226.983713	18.519872	-0.039206	2.021151
208.944665	1219.053009	18.524877	-0.039229	2.015621
208.691395	1211.143417	18.529882	-0.039176	2.010049
208.492374	1203.236368	18.534887	-0.039134	2.004468
208.511130	1195.331764	18.539891	-0.039132	1.998897
208.484499	1187.393288	18.544896	-0.039122	1.993281
208.394769	1179.454907	18.549901	-0.039100	1.987642
208.294175	1171.544002	18.554906	-0.039076	1.982006
208.379724	1163.620682	18.559911	-0.039087	1.976365
208.330245	1155.701687	18.564915	-0.039072	1.970697
208.026803	1147.796512	18.569920	-0.039010	1.964994
207.890776	1139.915446	18.574925	-0.038980	1.959311
208.030842	1131.955234	18.579930	-0.039001	1.953583
207.833391	1124.007477	18.584935	-0.038958	1.947811
207.833269	1116.085118	18.589939	-0.038953	1.942062
207.881073	1108.167413	18.594944	-0.038957	1.936305
207.868006	1100.234317	18.599949	-0.038949	1.930512
207.735311	1092.333265	18.604954	-0.038919	1.924712
207.491201	1084.456592	18.609959	-0.038868	1.918900
207.558733	1076.538421	18.614963	-0.038876	1.913074
207.317565	1068.629639	18.619968	-0.038826	1.907204
207.284256	1060.716601	18.624973	-0.038814	1.901335
207.116999	1052.824635	18.629978	-0.038778	1.895448
207.106026	1044.881088	18.634983	-0.038770	1.889522
207.056877	1036.995116	18.639987	-0.038756	1.883617
206.917135	1029.105116	18.644992	-0.038725	1.877679
206.969271	1021.173417	18.649997	-0.038729	1.871713
206.948081	1013.240984	18.655002	-0.038720	1.865719
206.844747	1005.342062	18.660007	-0.038696	1.859722
206.791920	997.458889	18.665011	-0.038680	1.853723
206.657101	989.550672	18.670016	-0.038650	1.847676
206.635361	981.655751	18.675021	-0.038641	1.841632
206.635259	973.757212	18.680026	-0.038636	1.835569
206.316001	965.876186	18.685031	-0.038571	1.829461
206.283423	957.978763	18.690035	-0.038560	1.823353
206.363217	950.060507	18.695040	-0.038569	1.817223
206.242137	942.175451	18.700045	-0.038541	1.811073
206.035892	934.303867	18.705050	-0.038498	1.804903
206.273365	926.373132	18.710055	-0.038537	1.798719
206.287373	918.459255	18.715059	-0.038534	1.792499
205.990734	910.552856	18.720064	-0.038474	1.786226
206.072580	902.654612	18.725069	-0.038484	1.779984
205.979775	894.790143	18.730074	-0.038461	1.773725
205.624112	886.920934	18.735079	-0.038390	1.767407
205.628406	879.042889	18.740083	-0.038385	1.761105
205.633910	871.148559	18.745088	-0.038381	1.754767
205.695597	863.238915	18.750093	-0.038387	1.748400
205.384202	855.401550	18.755098	-0.038324	1.742022
205.373313	847.505147	18.760103	-0.038317	1.735610
205.314870	839.628518	18.765107	-0.038301	1.729185
204.960724	831.790105	18.770112	-0.038229	1.722729
204.930324	823.914109	18.775117	-0.038218	1.716259
205.095681	815.981176	18.780122	-0.038244	1.709743
205.043035	808.098519	18.785127	-0.038229	1.703216
204.825593	800.259901	18.790131	-0.038183	1.696679
204.718445	792.372727	18.795136	-0.038158	1.690090
204.702634	784.501344	18.800141	-0.038150	1.683500
204.642130	776.652242	18.805146	-0.038133	1.676898
204.425407	768.779971	18.810151	-0.038088	1.670229
204.592991	760.891869	18.815155	-0.038114	1.663572
204.491632	753.038673	18.820160	-0.038090	1.656881
204.447021	745.154922	18.825165	-0.038076	1.650144
204.306034	737.328523	18.830170	-0.038045	1.643416
203.984878	729.503287	18.835175	-0.037980	1.636636
204.044878	721.581709	18.840179	-0.037986	1.629798
204.042002	713.697386	18.845184	-0.037980	1.622954
204.041818	705.848681	18.850189	-0.037975	1.616113
203.835888	698.014353	18.855194	-0.037931	1.609226
203.860414	690.149068	18.860199	-0.037930	1.602315
203.982293	682.298971	18.865203	-0.037948	1.595401
203.719960	674.467772	18.870208	-0.037894	1.588420
203.623033	666.643165	18.875213	-0.037871	1.581436
203.603702	658.808249	18.880218	-0.037862	1.574424
203.549243	650.953540	18.885223	-0.037846	1.567358
203.322152	643.150763	18.890227	-0.037799	1.560281
203.243921	635.309997	18.895232	-0.037779	1.553159
203.099215	627.461268	18.900237	-0.037747	1.545988
203.174975	619.617690	18.905242	-0.037756	1.538820
203.021385	611.788129	18.910247	-0.037722	1.531597
202.919287	603.977438	18.915251	-0.037698	1.524366
202.840561	596.158600	18.920256	-0.037678	1.517095
202.950110	588.302144	18.925261	-0.037693	1.509784
202.703253	580.521426	18.930266	-0.037642	1.502453
202.575802	572.705309	18.935271	-0.037613	1.495071
202.633795	564.866753	18.940275	-0.037619	1.487660
202.626479	557.046033	18.945280	-0.037612	1.480219
202.510101	549.243349	18.950285	-0.037585	1.472740
202.526876	541.392217	18.955290	-0.037583	1.465197
202.170966	533.642312	18.960295	-0.037512	1.457654
202.241819	525.815980	18.965299	-0.037520	1.450066
202.064648	518.035866	18.970304	-0.037482	1.442443
202.018953	510.252147	18.975309	-0.037468	1.434797
202.014210	502.440929	18.980314	-0.037462	1.427090
202.011740	494.646472	18.985319	-0.037456	1.419358
201.792816	486.898037	18.990323	-0.037410	1.411594
201.808443	479.090367	18.995328	-0.037408	1.403766
201.770548	471.327572	19.000333	-0.037396	1.395931
201.472341	463.573387	19.005338	-0.037335	1.388016
201.196695	455.822102	19.010343	-0.037279	1.380062
201.294687	448.033840	19.015347	-0.037292	1.372089
201.194172	440.257445	19.020352	-0.037268	1.364046
201.052522	432.519528	19.025357	-0.037236	1.355989
201.166282	424.728824	19.030362	-0.037252	1.347873
201.094564	416.977085	19.035367	-0.037234	1.339717
200.865742	409.257282	19.040371	-0.037186	1.331516
200.779601	401.509585	19.045376	-0.037165	1.323260
200.921525	393.737281	19.050381	-0.037186	1.314967
200.771890	385.896686	19.055386	-0.037153	1.306494
200.424986	378.219745	19.060391	-0.037083	1.298109
200.631745	370.456518	19.065395	-0.037117	1.289676
200.547792	362.742494	19.070400	-0.037096	1.281187
200.290283	355.078631	19.075405	-0.037043	1.272666
200.077401	347.389102	19.080410	-0.036998	1.264066
200.079314	339.670832	19.085415	-0.036993	1.255416
200.130378	331.952036	19.090419	-0.036998	1.246715
199.999999	324.283648	19.095424	-0.036968	1.237975
199.987059	316.572719	19.100429	-0.036961	1.229147
199.919984	308.886867	19.105434	-0.036943	1.220274
199.517525	301.266274	19.110439	-0.036863	1.211345
199.454904	293.595503	19.115443	-0.036846	1.202358
199.432157	285.924375	19.120448	-0.036837	1.193311
199.481658	278.240321	19.125453	-0.036841	1.184195
199.477410	270.590976	19.130458	-0.036835	1.175038
199.316233	262.949278	19.135463	-0.036800	1.165787
199.309122	255.332073	19.140467	-0.036794	1.156523
198.983194	247.694927	19.145472	-0.036728	1.147093
198.952103	240.072428	19.150477	-0.036717	1.137665
198.788450	232.468357	19.155482	-0.036682	1.128153
198.695104	224.863365	19.160487	-0.036659	1.118574
198.534566	217.286038	19.165491	-0.036624	1.108933
198.539086	209.672789	19.170496	-0.036620	1.099198
198.361059	202.114836	19.175501	-0.036582	1.089407
198.290684	194.555918	19.180506	-0.036564	1.079549
198.189393	186.986286	19.185511	-0.036540	1.069580
198.165671	179.429048	19.190515	-0.036530	1.059551
197.916309	171.907571	19.195520	-0.036479	1.049422
197.712350	164.404632	19.200525	-0.036436	1.039230
197.754295	156.869617	19.205530	-0.036439	1.028951
197.357281	149.411256	19.210535	-0.036360	1.018569
197.158327	141.934049	19.215539	-0.036318	1.008102
196.901275	134.480328	19.220544	-0.036265	0.997544
196.822782	126.968999	19.225549	-0.036245	0.986835
196.422086	119.563381	19.230554	-0.036166	0.976080
196.167498	112.127740	19.235559	-0.036114	0.965198
195.782860	104.756159	19.240563	-0.036037	0.954253
195.126719	97.413866	19.245568	-0.035910	0.943154
194.902943	90.025978	19.250573	-0.035863	0.931968
194.498176	82.683296	19.255578	-0.035783	0.920666
193.944051	75.363185	19.260583	-0.035675	0.909218
193.664512	68.027931	19.265587	-0.035618	0.897676
193.358948	60.931302	19.270592	-0.035557	0.886356