Thu Mar 11 20:13:56 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.734938	-0.033226	0.000000	0.000003	0.721223

0.778514	-0.089827	0.005005	-0.000005	0.721127
0.465277	-0.035469	0.010010	0.000053	0.721125
0.653943	-0.064138	0.015014	0.000018	0.721134
0.512223	-0.043696	0.020019	0.000044	0.721125
0.728863	-0.079846	0.025024	0.000004	0.721130
0.716917	-0.079140	0.030029	0.000006	0.721127
0.589600	-0.059517	0.035034	0.000030	0.721121
0.601071	-0.057664	0.040038	0.000028	0.721129
0.500300	-0.043005	0.045043	0.000047	0.721122
0.773465	-0.089103	0.050048	-0.000004	0.721128
0.667678	-0.070139	0.055053	0.000015	0.721128
0.640817	-0.068919	0.060058	0.000020	0.721121
0.869471	-0.104789	0.065062	-0.000022	0.721130
0.754985	-0.089037	0.070067	-0.000001	0.721121
0.682704	-0.073381	0.075072	0.000012	0.721127
0.601235	-0.122427	0.080077	0.000028	0.721002
0.409032	-0.153566	0.085082	0.000063	0.720873
0.684074	-0.198214	0.090086	0.000012	0.720882
0.600723	-0.186617	0.095091	0.000028	0.720876
0.633925	-0.190023	0.100096	0.000021	0.720881
0.531436	-0.171924	0.105101	0.000040	0.720880
0.363746	-0.144594	0.110106	0.000072	0.720876
0.552117	-0.301349	0.115110	0.000037	0.720633
0.460178	-0.334451	0.120115	0.000054	0.720536
0.577734	-0.352405	0.125120	0.000032	0.720542
0.726411	-0.379073	0.130125	0.000004	0.720541
0.563392	-0.351779	0.135130	0.000034	0.720538
0.512988	-0.446813	0.140134	0.000044	0.720333
0.570238	-0.512526	0.145139	0.000033	0.720224
0.743663	-0.540946	0.150144	0.000001	0.720229
0.488705	-0.497239	0.155149	0.000048	0.720226
0.284663	-0.533052	0.160154	0.000086	0.720084
0.386711	-0.642296	0.165158	0.000067	0.719904
0.247134	-0.622106	0.170163	0.000093	0.719895
0.288444	-0.626247	0.175168	0.000085	0.719902
0.299093	-0.694320	0.180173	0.000084	0.719771
0.221600	-0.767907	0.185178	0.000098	0.719599
0.257487	-0.771164	0.190182	0.000091	0.719605
0.196452	-0.765672	0.195187	0.000103	0.719595
0.287803	-0.924167	0.200192	0.000086	0.719314
0.195658	-0.930902	0.205197	0.000103	0.719269
0.449018	-0.978432	0.210202	0.000056	0.719264
0.436079	-1.073781	0.215206	0.000058	0.719072
0.199009	-1.089273	0.220211	0.000102	0.718958
0.411489	-1.126397	0.225216	0.000063	0.718959
0.430912	-1.241468	0.230221	0.000059	0.718739
0.194404	-1.249243	0.235226	0.000103	0.718641
0.299023	-1.263124	0.240230	0.000083	0.718650
0.310826	-1.405567	0.245235	0.000081	0.718373
0.423822	-1.436081	0.250240	0.000060	0.718353
0.450637	-1.496261	0.255245	0.000055	0.718243
0.367611	-1.596529	0.260250	0.000071	0.718016
0.544739	-1.625859	0.265254	0.000038	0.718021
0.088082	-1.692006	0.270259	0.000123	0.717729
0.169953	-1.719613	0.275264	0.000108	0.717704
0.248771	-1.811471	0.280269	0.000093	0.717550
-0.052313	-1.846145	0.285274	0.000149	0.717375
0.348225	-1.933704	0.290278	0.000074	0.717343
0.200525	-2.040142	0.295283	0.000102	0.717081
0.200502	-2.038434	0.300288	0.000102	0.717084
0.119820	-2.181292	0.305293	0.000117	0.716773
-0.001209	-2.171953	0.310298	0.000139	0.716749
-0.141785	-2.262083	0.315302	0.000166	0.716521
-1.582494	-2.043168	0.320307	0.000434	0.716447
-1.308880	-2.146728	0.325312	0.000383	0.716338
-2.573836	-2.025345	0.330317	0.000618	0.716132
-2.627358	-2.018247	0.335322	0.000628	0.716127
-2.366026	-2.110928	0.340326	0.000580	0.716036
-3.423040	-2.002473	0.345331	0.000776	0.715878
-3.240567	-2.032923	0.350336	0.000742	0.715882
-3.129345	-2.096643	0.355341	0.000722	0.715795
-4.370154	-2.002933	0.360346	0.000953	0.715543
-4.073639	-2.051260	0.365350	0.000897	0.715552
-4.845357	-1.919249	0.370355	0.001041	0.715541
-4.684532	-2.047475	0.375360	0.001011	0.715344
-5.473582	-1.963530	0.380365	0.001158	0.715231
-5.426628	-1.974957	0.385370	0.001149	0.715225
-4.901077	-2.064444	0.390374	0.001051	0.715234
-5.610540	-2.011426	0.395379	0.001183	0.715088
-6.834309	-1.882578	0.400384	0.001411	0.714911
-6.050395	-2.022305	0.405389	0.001265	0.714911
-6.592036	-1.931546	0.410394	0.001366	0.714900
-6.546383	-1.935032	0.415398	0.001357	0.714909
-6.307429	-2.057387	0.420403	0.001313	0.714751
-7.098654	-1.989157	0.425408	0.001460	0.714607
-6.986954	-2.009836	0.430413	0.001439	0.714605
-7.370457	-1.942883	0.435418	0.001511	0.714603
-7.215441	-1.965579	0.440422	0.001482	0.714612
-7.191150	-2.067146	0.445427	0.001477	0.714419
-8.577723	-1.891200	0.450432	0.001735	0.714278
-8.040349	-1.987599	0.455437	0.001635	0.714277
-8.177339	-1.965623	0.460442	0.001661	0.714272
-8.131377	-1.968618	0.465446	0.001652	0.714283
-8.313125	-1.941222	0.470451	0.001686	0.714273
-8.631524	-2.004666	0.475456	0.001745	0.714034
-9.371754	-1.905575	0.480461	0.001883	0.713969
-9.292729	-1.921768	0.485466	0.001868	0.713965
-8.669269	-2.028990	0.490470	0.001752	0.713973
-9.150608	-1.946604	0.495475	0.001842	0.713966
-9.166144	-1.941905	0.500480	0.001845	0.713970
-9.030415	-2.054833	0.505485	0.001819	0.713794
-10.239671	-1.914524	0.510490	0.002044	0.713644
-9.694463	-2.005571	0.515494	0.001943	0.713656
-9.964126	-1.961366	0.520499	0.001993	0.713649
-10.045874	-1.943066	0.525504	0.002008	0.713656
-9.915679	-1.966098	0.530509	0.001984	0.713657
-10.274048	-1.948602	0.535514	0.002051	0.713565
-10.783524	-1.960962	0.540518	0.002145	0.713360
-10.362939	-2.037696	0.545523	0.002067	0.713356
-10.997173	-1.923040	0.550528	0.002185	0.713359
-10.885834	-1.943420	0.555533	0.002164	0.713358
-10.772161	-1.966335	0.560538	0.002143	0.713353
-10.926287	-1.933178	0.565542	0.002172	0.713365
-11.510098	-1.976234	0.570547	0.002281	0.713072
-12.073003	-1.900054	0.575552	0.002385	0.713024
-11.921362	-1.927772	0.580557	0.002357	0.713023
-11.836281	-1.945043	0.585562	0.002341	0.713019
-11.620231	-1.977530	0.590566	0.002301	0.713031
-11.923854	-1.928564	0.595571	0.002357	0.713021
-12.020528	-1.909371	0.600576	0.002375	0.713024
-11.962300	-2.020445	0.605581	0.002365	0.712824
-12.850138	-1.921368	0.610586	0.002530	0.712707
-12.507898	-1.979950	0.615590	0.002466	0.712711
-12.760772	-1.936455	0.620595	0.002513	0.712708
-12.443283	-1.991176	0.625600	0.002454	0.712712
-12.201786	-2.034395	0.630605	0.002409	0.712712
-12.897398	-1.919187	0.635610	0.002538	0.712694
-13.270186	-2.004553	0.640614	0.002608	0.712392
-13.130012	-2.034578	0.645619	0.002582	0.712382
-13.884081	-1.899073	0.650624	0.002722	0.712385
-13.802879	-1.910597	0.655629	0.002707	0.712390
-13.792366	-1.915402	0.660634	0.002705	0.712385
-13.654272	-1.936828	0.665638	0.002679	0.712391
-13.593900	-1.952006	0.670643	0.002668	0.712382
-13.934189	-2.019944	0.675648	0.002731	0.712126
-14.359006	-1.962415	0.680653	0.002810	0.712090
-14.863869	-1.875073	0.685658	0.002904	0.712085
-14.379990	-1.956039	0.690662	0.002814	0.712096
-14.483051	-1.943935	0.695667	0.002833	0.712083
-14.729508	-1.896567	0.700672	0.002879	0.712090
-14.306446	-1.968967	0.705677	0.002800	0.712096
-14.759834	-2.020456	0.710682	0.002885	0.711833
-15.383820	-1.942774	0.715686	0.003001	0.711766
-15.673959	-1.894317	0.720691	0.003055	0.711759
-15.379039	-1.947332	0.725696	0.003000	0.711759
-15.299041	-1.958136	0.730701	0.002985	0.711765
-15.821309	-1.868824	0.735706	0.003082	0.711758
-15.593880	-1.904685	0.740710	0.003040	0.711767
-15.354692	-2.010832	0.745715	0.002995	0.711641
-16.294351	-1.935902	0.750720	0.003170	0.711456
-16.174570	-1.956066	0.755725	0.003148	0.711459
-16.765842	-1.855433	0.760730	0.003258	0.711449
-16.160217	-1.959902	0.765734	0.003145	0.711456
-16.148921	-1.963983	0.770739	0.003143	0.711452
-16.505509	-1.900630	0.775744	0.003209	0.711452
-16.250871	-1.993108	0.780749	0.003162	0.711358
-17.151694	-1.944496	0.785754	0.003330	0.711135
-16.994525	-1.968430	0.790758	0.003300	0.711143
-17.213528	-1.933621	0.795763	0.003341	0.711135
-17.230139	-1.929442	0.800768	0.003344	0.711137
-16.950915	-1.976768	0.805773	0.003292	0.711142
-17.197163	-1.937457	0.810778	0.003338	0.711133
-17.189288	-1.998143	0.815782	0.003336	0.711015
-18.391322	-1.857286	0.820787	0.003560	0.710869
-17.979180	-1.929278	0.825792	0.003483	0.710871
-17.485267	-2.016975	0.830797	0.003391	0.710872
-18.161656	-1.899015	0.835802	0.003517	0.710867
-18.110641	-1.905480	0.840806	0.003508	0.710872
-18.113204	-1.907675	0.845811	0.003508	0.710867
-18.100816	-1.982393	0.850816	0.003506	0.710722
-19.032876	-1.909072	0.855821	0.003679	0.710537
-19.120263	-1.898104	0.860826	0.003696	0.710528
-18.755328	-1.959419	0.865830	0.003628	0.710536
-18.795747	-1.955101	0.870835	0.003635	0.710530
-19.097853	-1.899929	0.875840	0.003691	0.710533
-18.891410	-1.935775	0.880845	0.003653	0.710535
-19.123355	-1.938159	0.885850	0.003696	0.710447
-19.662479	-1.954430	0.890854	0.003796	0.710223
-19.686668	-1.955034	0.895859	0.003801	0.710213
-20.123644	-1.877076	0.900864	0.003882	0.710213
-19.608256	-1.966300	0.905869	0.003786	0.710219
-19.864769	-1.924760	0.910874	0.003834	0.710210
-19.686347	-1.952410	0.915878	0.003801	0.710219
-19.891784	-1.957974	0.920883	0.003839	0.710135
-20.890042	-1.902011	0.925888	0.004025	0.709891
-20.165086	-2.030928	0.930893	0.003890	0.709892
-20.941100	-1.893485	0.935898	0.004034	0.709890
-21.079004	-1.866481	0.940902	0.004060	0.709895
-21.076686	-1.868176	0.945907	0.004059	0.709892
-20.712001	-1.932225	0.950912	0.003991	0.709894
-20.450672	-1.978244	0.955917	0.003943	0.709895
-21.494321	-1.944624	0.960922	0.004137	0.709591
-21.496642	-1.939444	0.965926	0.004137	0.709600
-21.737821	-1.899109	0.970931	0.004182	0.709595
-21.380962	-1.962310	0.975936	0.004116	0.709596
-21.521382	-1.934937	0.980941	0.004142	0.709601
-21.654789	-1.915682	0.985946	0.004167	0.709592
-21.496577	-1.946760	0.990950	0.004137	0.709586
-22.327304	-1.961466	0.995955	0.004292	0.709261
-22.396719	-1.948581	1.000960	0.004305	0.709262
-22.851483	-1.863587	1.005965	0.004389	0.709270
-22.636787	-1.906798	1.010970	0.004349	0.709260
-22.190739	-1.981957	1.015974	0.004266	0.709269
-22.558669	-1.918172	1.020979	0.004335	0.709265
-22.586572	-1.913154	1.025984	0.004340	0.709265
-22.541993	-2.041907	1.030989	0.004332	0.709023
-23.370003	-1.928404	1.035994	0.004486	0.708955
-23.536166	-1.895665	1.040998	0.004517	0.708962
-23.449671	-1.913725	1.046003	0.004500	0.708956
-23.248383	-1.949243	1.051008	0.004463	0.708957
-22.929917	-2.005137	1.056013	0.004404	0.708959
-23.390414	-1.937094	1.061018	0.004489	0.708931
-24.164393	-1.943162	1.066022	0.004633	0.708643
-24.149869	-1.949875	1.071027	0.004631	0.708634
-24.549316	-1.876376	1.076032	0.004705	0.708639
-24.134548	-1.947449	1.081037	0.004628	0.708645
-24.265593	-1.925724	1.086042	0.004652	0.708642
-24.383744	-1.900529	1.091046	0.004674	0.708650
-24.319476	-1.916575	1.096051	0.004662	0.708641
-24.474752	-2.006753	1.101056	0.004691	0.708405
-25.108404	-1.917999	1.106061	0.004809	0.708357
-25.484000	-1.856113	1.111066	0.004879	0.708346
-24.809940	-1.971144	1.116070	0.004753	0.708357
-25.064061	-1.928026	1.121075	0.004801	0.708352
-25.340811	-1.878188	1.126080	0.004852	0.708354
-24.975701	-1.941192	1.131085	0.004784	0.708358
-25.395464	-2.015056	1.136090	0.004862	0.708060
-26.222346	-1.887564	1.141094	0.005016	0.708020
-26.367513	-1.865382	1.146099	0.005043	0.708013
-25.824918	-1.961230	1.151104	0.004942	0.708015
-25.732765	-1.973600	1.156109	0.004925	0.708023
-26.359463	-1.868511	1.161114	0.005041	0.708010
-26.150085	-1.902320	1.166118	0.005002	0.708017
-26.395049	-1.952154	1.171123	0.005048	0.707829
-27.404338	-1.836661	1.176128	0.005236	0.707700
-26.884469	-1.925269	1.181133	0.005139	0.707708
-27.040927	-1.903213	1.186138	0.005168	0.707697
-27.127596	-1.882350	1.191142	0.005184	0.707708
-26.862452	-1.931238	1.196147	0.005135	0.707704
-26.907868	-1.924148	1.201152	0.005143	0.707702
-26.940887	-1.967441	1.206157	0.005149	0.707604
-28.236672	-1.852746	1.211162	0.005391	0.707371
-27.556933	-1.967910	1.216166	0.005264	0.707383
-27.621881	-1.958700	1.221171	0.005276	0.707378
-28.171530	-1.860177	1.226176	0.005378	0.707379
-27.808102	-1.923316	1.231181	0.005311	0.707383
-27.758371	-1.936336	1.236186	0.005301	0.707374
-27.873692	-1.950584	1.241190	0.005323	0.707305
-28.723169	-1.911499	1.246195	0.005481	0.707079
-28.394034	-1.968334	1.251200	0.005420	0.707083
-28.352240	-1.973445	1.256205	0.005412	0.707088
-28.709294	-1.914265	1.261210	0.005478	0.707079
-28.604497	-1.929479	1.266214	0.005459	0.707086
-28.737577	-1.908123	1.271219	0.005483	0.707081
-28.831260	-1.959331	1.276224	0.005501	0.706945
-29.555175	-1.922980	1.281229	0.005636	0.706759
-29.478720	-1.942314	1.286234	0.005621	0.706747
-29.674484	-1.902128	1.291238	0.005658	0.706758
-29.678412	-1.904530	1.296243	0.005658	0.706752
-29.400836	-1.953497	1.301248	0.005607	0.706753
-29.383893	-1.955112	1.306253	0.005604	0.706756
-29.815648	-1.943928	1.311258	0.005684	0.706624
-30.553697	-1.900038	1.316262	0.005821	0.706448
-30.079487	-1.987437	1.321267	0.005733	0.706442
-30.686089	-1.879106	1.326272	0.005846	0.706443
-30.537373	-1.901919	1.331277	0.005818	0.706450
-30.277038	-1.953835	1.336282	0.005770	0.706439
-30.495410	-1.911174	1.341286	0.005810	0.706447
-30.782817	-1.902270	1.346291	0.005864	0.706362
-31.570361	-1.879144	1.351296	0.006010	0.706126
-30.960694	-1.984789	1.356301	0.005897	0.706132
-31.802736	-1.838174	1.361306	0.006054	0.706125
-31.588803	-1.874013	1.366310	0.006014	0.706130
-31.213493	-1.942269	1.371315	0.005944	0.706127
-31.325894	-1.922498	1.376320	0.005965	0.706127
-31.358046	-1.915751	1.381325	0.005971	0.706129
-31.879523	-1.957437	1.386330	0.006068	0.705858
-32.036864	-1.924571	1.391334	0.006097	0.705868
-32.017103	-1.930299	1.396339	0.006093	0.705864
-31.986248	-1.937812	1.401344	0.006088	0.705860
-32.003275	-1.930113	1.406349	0.006091	0.705869
-32.336457	-1.875370	1.411354	0.006153	0.705860
-32.070277	-1.989945	1.416358	0.006103	0.705725
-33.103711	-1.905415	1.421363	0.006295	0.705524
-33.064741	-1.912821	1.426368	0.006288	0.705523
-33.135776	-1.896583	1.431373	0.006301	0.705531
-32.992666	-1.926123	1.436378	0.006275	0.705523
-32.682751	-1.976012	1.441382	0.006217	0.705533
-33.082946	-1.908155	1.446387	0.006291	0.705527
-33.411723	-1.940447	1.451392	0.006353	0.705344
-33.610570	-1.968117	1.456397	0.006390	0.705217
-33.797762	-1.939742	1.461402	0.006424	0.705207
-34.055940	-1.890027	1.466406	0.006472	0.705214
-34.031805	-1.895603	1.471411	0.006468	0.705212
-33.863892	-1.926074	1.476416	0.006437	0.705211
-34.025895	-1.894473	1.481421	0.006467	0.705216
-34.164252	-1.968265	1.486426	0.006492	0.705018
-34.877918	-1.904668	1.491430	0.006625	0.704890
-34.861330	-1.908743	1.496435	0.006622	0.704888
-34.776899	-1.923711	1.501440	0.006606	0.704888
-34.639569	-1.945785	1.506445	0.006581	0.704893
-34.999576	-1.885900	1.511450	0.006648	0.704884
-34.991463	-1.884589	1.516454	0.006646	0.704890
-34.905834	-1.961188	1.521459	0.006630	0.704766
-35.805074	-1.889658	1.526464	0.006798	0.704588
-35.630409	-1.916957	1.531469	0.006765	0.704595
-35.820451	-1.887215	1.536474	0.006800	0.704587
-35.298484	-1.977476	1.541478	0.006703	0.704593
-35.644354	-1.916622	1.546483	0.006768	0.704591
-36.187083	-1.821989	1.551488	0.006869	0.704587
-35.570112	-2.002621	1.556493	0.006754	0.704445
-36.611764	-1.910109	1.561498	0.006948	0.704257
-36.778077	-1.875535	1.566502	0.006979	0.704267
-36.597041	-1.909896	1.571507	0.006945	0.704263
-36.541138	-1.921831	1.576512	0.006934	0.704259
-36.206186	-1.977902	1.581517	0.006872	0.704266
-36.928515	-1.854033	1.586522	0.007006	0.704257
-36.547121	-1.987331	1.591526	0.006935	0.704125
-37.372961	-1.924888	1.596531	0.007089	0.703954
-37.312174	-1.938854	1.601536	0.007078	0.703948
-37.213840	-1.952549	1.606541	0.007059	0.703956
-37.462199	-1.912791	1.611546	0.007106	0.703947
-37.519252	-1.899595	1.616550	0.007116	0.703953
-37.405176	-1.918921	1.621555	0.007095	0.703955
-37.512885	-2.001860	1.626560	0.007115	0.703749
-38.563043	-1.869667	1.631565	0.007310	0.703638
-38.538145	-1.877118	1.636570	0.007306	0.703632
-37.934716	-1.981874	1.641574	0.007194	0.703638
-38.174046	-1.940320	1.646579	0.007238	0.703635
-38.637152	-1.860299	1.651584	0.007324	0.703630
-38.002387	-1.967780	1.656589	0.007206	0.703642
-38.115665	-2.050220	1.661594	0.007227	0.703435
-39.472788	-1.853602	1.666598	0.007480	0.703343
-39.421503	-1.864364	1.671603	0.007470	0.703340
-39.219832	-1.900779	1.676608	0.007433	0.703339
-38.899558	-1.954010	1.681613	0.007373	0.703347
-39.074389	-1.926737	1.686618	0.007405	0.703339
-39.092328	-1.920362	1.691622	0.007409	0.703346
-39.288808	-2.017180	1.696627	0.007445	0.703080
-40.365275	-1.860796	1.701632	0.007646	0.703008
-39.924876	-1.934289	1.706637	0.007564	0.703018
-39.847741	-1.953949	1.711642	0.007549	0.703006
-40.105134	-1.904147	1.716646	0.007597	0.703014
-39.972286	-1.930223	1.721651	0.007572	0.703010
-39.848867	-1.954194	1.726656	0.007549	0.703006
-40.469021	-1.989849	1.731661	0.007665	0.702710
-41.191254	-1.871728	1.736666	0.007799	0.702689
-40.912408	-1.916960	1.741670	0.007747	0.702698
-40.372739	-2.014183	1.746675	0.007647	0.702696
-41.277851	-1.855343	1.751680	0.007815	0.702691
-40.922079	-1.914755	1.756685	0.007749	0.702699
-40.578953	-1.982264	1.761690	0.007685	0.702686
-41.327555	-2.002396	1.766694	0.007824	0.702376
-41.851262	-1.910052	1.771699	0.007922	0.702374
-41.973863	-1.889807	1.776704	0.007945	0.702371
-41.411816	-1.987277	1.781709	0.007840	0.702376
-42.050897	-1.877449	1.786714	0.007959	0.702368
-41.973346	-1.888685	1.791718	0.007944	0.702373
-41.634266	-1.949139	1.796723	0.007881	0.702374
-42.548616	-1.931731	1.801728	0.008051	0.702079
-42.745559	-1.895141	1.806733	0.008088	0.702082
-42.596639	-1.926629	1.811738	0.008060	0.702072
-42.621472	-1.919880	1.816742	0.008065	0.702077
-42.884536	-1.873353	1.821747	0.008114	0.702076
-42.656281	-1.916941	1.826752	0.008071	0.702071
-42.304318	-1.975256	1.831757	0.008006	0.702080
-43.650601	-1.891330	1.836762	0.008256	0.701764
-43.724598	-1.886500	1.841766	0.008270	0.701747
-43.365178	-1.952512	1.846771	0.008203	0.701743
-43.681597	-1.897820	1.851776	0.008262	0.701740
-43.793801	-1.873371	1.856781	0.008283	0.701749
-43.544058	-1.922488	1.861786	0.008236	0.701740
-43.416274	-1.943416	1.866790	0.008213	0.701743
-43.830002	-1.960189	1.871795	0.008290	0.701560
-44.942518	-1.825382	1.876800	0.008497	0.701432
-44.113901	-1.969433	1.881805	0.008342	0.701439
-44.524455	-1.901037	1.886810	0.008419	0.701429
-44.659611	-1.873229	1.891814	0.008444	0.701437
-44.362352	-1.927579	1.896819	0.008389	0.701434
-44.445612	-1.915811	1.901824	0.008404	0.701428
-44.407537	-1.996801	1.906829	0.008397	0.701278
-45.385035	-1.901763	1.911834	0.008579	0.701118
-45.216845	-1.929013	1.916838	0.008548	0.701123
-45.241810	-1.925788	1.921843	0.008552	0.701121
-45.359807	-1.907246	1.926848	0.008574	0.701116
-44.787000	-2.004683	1.931853	0.008467	0.701125
-45.240991	-1.929655	1.936858	0.008552	0.701113
-45.572290	-1.970438	1.941862	0.008614	0.700911
-45.455476	-2.010486	1.946867	0.008592	0.700872
-45.834888	-1.944478	1.951872	0.008662	0.700869
-45.950523	-1.919653	1.956877	0.008684	0.700878
-46.062876	-1.904349	1.961882	0.008705	0.700868
-45.520499	-1.997750	1.966886	0.008604	0.700875
-46.173232	-2.004668	1.971891	0.008725	0.700625
-47.419453	-1.829168	1.976896	0.008957	0.700530
-46.711310	-1.949478	1.981901	0.008825	0.700543
-46.793122	-1.941620	1.986906	0.008841	0.700529
-47.052011	-1.892059	1.991910	0.008889	0.700536
-46.833431	-1.931456	1.996915	0.008848	0.700535
-46.886838	-1.979274	2.001920	0.008858	0.700419

-47.761955	-1.924210	2.011917	0.009021	0.700214
-47.954095	-1.888854	2.021914	0.009056	0.700217
-47.773067	-1.919277	2.031910	0.009023	0.700221
-47.824412	-1.910609	2.041907	0.009032	0.700220
-47.937499	-1.891162	2.051904	0.009053	0.700218
-47.786855	-1.919364	2.061901	0.009025	0.700216
-47.939656	-1.892719	2.071898	0.009053	0.700215
-47.724286	-1.929921	2.081894	0.009013	0.700217
-47.819343	-1.913073	2.091891	0.009031	0.700217
-47.805086	-1.905469	2.101888	0.009028	0.700238
-47.100782	-1.885831	2.111885	0.008897	0.700533
-46.813252	-1.936901	2.121882	0.008843	0.700533
-46.802239	-1.939162	2.131878	0.008841	0.700533
-46.904088	-1.920949	2.141875	0.008860	0.700533
-46.911817	-1.921448	2.151872	0.008862	0.700529
-46.962197	-1.913300	2.161869	0.008871	0.700528
-46.237064	-1.912582	2.171866	0.008736	0.700791
-46.084745	-1.900278	2.181862	0.008707	0.700871
-45.852895	-1.941264	2.191859	0.008664	0.700872
-45.947338	-1.925413	2.201856	0.008682	0.700870
-46.115648	-1.882157	2.211853	0.008713	0.700897
-45.394277	-1.901067	2.221850	0.008578	0.701120
-45.390275	-1.901268	2.231846	0.008578	0.701121
-45.299021	-1.917760	2.241843	0.008561	0.701121
-45.123282	-1.883525	2.251840	0.008528	0.701254
-44.374715	-1.927451	2.261837	0.008388	0.701435
-44.429273	-1.918096	2.271834	0.008398	0.701434
-44.500986	-1.904486	2.281830	0.008412	0.701436
-43.833208	-1.908572	2.291827	0.008287	0.701669
-43.813782	-1.875143	2.301824	0.008284	0.701744
-43.620380	-1.909772	2.311821	0.008248	0.701744
-43.558600	-1.873077	2.321818	0.008236	0.701840
-42.478814	-1.952642	2.331814	0.008035	0.702069
-42.767152	-1.899710	2.341811	0.008088	0.702072
-42.729128	-1.906478	2.351808	0.008081	0.702072
-42.362049	-1.864060	2.361805	0.008013	0.702291
-41.878211	-1.911820	2.371802	0.007923	0.702369
-41.815784	-1.921355	2.381798	0.007911	0.702372
-41.774564	-1.893977	2.391795	0.007903	0.702442
-40.972658	-1.910852	2.401792	0.007754	0.702697
-41.007716	-1.907876	2.411789	0.007760	0.702691
-41.134023	-1.885150	2.421786	0.007784	0.702691
-40.443156	-1.886240	2.431782	0.007655	0.702938
-40.131170	-1.907459	2.441779	0.007597	0.703008
-40.042507	-1.923062	2.451776	0.007580	0.703008
-40.176502	-1.851950	2.461773	0.007605	0.703104
-39.132587	-1.920322	2.471770	0.007411	0.703342
-39.250606	-1.898880	2.481766	0.007433	0.703343
-39.159263	-1.914767	2.491763	0.007416	0.703344
-38.556063	-1.914005	2.501760	0.007303	0.703562
-38.199575	-1.940722	2.511757	0.007237	0.703637
-38.226398	-1.937476	2.521754	0.007242	0.703634
-38.206272	-1.939116	2.531750	0.007238	0.703638
-37.664132	-1.880575	2.541747	0.007137	0.703951
-37.366126	-1.933461	2.551744	0.007081	0.703952
-37.707706	-1.872782	2.561741	0.007145	0.703952
-36.944569	-1.911440	2.571738	0.007003	0.704148
-36.875680	-1.865605	2.581734	0.006990	0.704265
-36.474793	-1.938847	2.591731	0.006915	0.704262
-36.595480	-1.885142	2.601728	0.006938	0.704327
-35.746551	-1.907274	2.611725	0.006779	0.704587
-35.770742	-1.902910	2.621722	0.006784	0.704588
-35.430719	-1.963129	2.631718	0.006720	0.704589
-35.280695	-1.904021	2.641715	0.006692	0.704762
-34.844523	-1.917247	2.651712	0.006611	0.704892
-35.110047	-1.872537	2.661709	0.006661	0.704887
-34.721662	-1.910528	2.671706	0.006588	0.704950
-34.063019	-1.896980	2.681702	0.006465	0.705214
-33.742978	-1.954604	2.691699	0.006406	0.705213
-34.081654	-1.894487	2.701696	0.006469	0.705212
-33.441107	-1.898242	2.711693	0.006349	0.705435
-33.071442	-1.920284	2.721690	0.006281	0.705523
-33.069287	-1.917471	2.731686	0.006280	0.705530
-33.014845	-1.903472	2.741683	0.006270	0.705577
-32.078018	-1.925903	2.751680	0.006095	0.705868
-31.896409	-1.961218	2.761677	0.006062	0.705863
-31.968253	-1.947466	2.771674	0.006075	0.705865
-32.158377	-1.867784	2.781670	0.006110	0.705957
-31.109063	-1.968808	2.791667	0.005915	0.706130
-31.487181	-1.902247	2.801664	0.005985	0.706128
-31.678805	-1.852449	2.811661	0.006021	0.706160
-30.630626	-1.897866	2.821658	0.005825	0.706444
-30.502328	-1.920529	2.831654	0.005801	0.706445
-30.561882	-1.908539	2.841651	0.005812	0.706448
-29.994636	-1.884348	2.851648	0.005707	0.706700
-29.712967	-1.907776	2.861645	0.005654	0.706754
-29.527829	-1.941426	2.871642	0.005620	0.706752
-29.510237	-1.891629	2.881638	0.005616	0.706859
-28.481507	-1.962854	2.891635	0.005425	0.707084
-28.849128	-1.899376	2.901632	0.005493	0.707080
-28.775982	-1.912713	2.911629	0.005479	0.707080
-28.200919	-1.892364	2.921626	0.005372	0.707326
-28.047019	-1.895171	2.931622	0.005344	0.707376
-27.811621	-1.936182	2.941619	0.005300	0.707378
-27.762738	-1.873021	2.951616	0.005290	0.707522
-26.869784	-1.943501	2.961613	0.005124	0.707700
-27.380846	-1.853331	2.971610	0.005219	0.707699
-27.087895	-1.893494	2.981606	0.005165	0.707723
-26.370384	-1.876506	2.991603	0.005031	0.708014
-26.236850	-1.899670	3.001600	0.005006	0.708015
-26.036556	-1.936137	3.011597	0.004969	0.708014
-25.881972	-1.861958	3.021594	0.004940	0.708218
-25.119363	-1.930597	3.031590	0.004798	0.708353
-25.355400	-1.888593	3.041587	0.004842	0.708353
-25.467036	-1.843410	3.051584	0.004862	0.708403
-24.540572	-1.889967	3.061581	0.004690	0.708641
-24.615815	-1.877558	3.071578	0.004704	0.708639
-24.392794	-1.917919	3.081574	0.004662	0.708638
-24.042772	-1.854746	3.091571	0.004597	0.708890
-23.733134	-1.875296	3.101568	0.004539	0.708959
-23.458290	-1.926414	3.111565	0.004488	0.708955
-23.548998	-1.859406	3.121562	0.004505	0.709057
-22.791833	-1.890314	3.131558	0.004364	0.709265
-22.623843	-1.920553	3.141555	0.004332	0.709265
-22.801202	-1.889595	3.151552	0.004365	0.709264
-22.078837	-1.868400	3.161549	0.004231	0.709564
-22.026764	-1.862195	3.171546	0.004221	0.709595
-21.507805	-1.954084	3.181542	0.004124	0.709596
-21.899690	-1.817760	3.191539	0.004197	0.709729
-20.684755	-1.950350	3.201536	0.003971	0.709897
-21.139025	-1.871569	3.211533	0.004055	0.709893
-20.861055	-1.920313	3.221530	0.004004	0.709895
-20.097956	-1.924846	3.231526	0.003861	0.710158
-20.095201	-1.894859	3.241523	0.003861	0.710219
-20.187061	-1.878749	3.251520	0.003878	0.710218
-19.955953	-1.880029	3.261517	0.003835	0.710298
-19.375751	-1.864564	3.271514	0.003727	0.710536
-19.161750	-1.902179	3.281510	0.003687	0.710537
-19.483671	-1.844759	3.291507	0.003747	0.710537
-18.421779	-1.877082	3.301504	0.003549	0.710851
-18.531850	-1.846297	3.311501	0.003569	0.710873
-18.193622	-1.906126	3.321498	0.003506	0.710874
-18.152179	-1.862761	3.331494	0.003498	0.710975
-17.511347	-1.892559	3.341491	0.003379	0.711144
-17.594024	-1.879184	3.351488	0.003394	0.711141
-17.747197	-1.847333	3.361485	0.003423	0.711151
-16.997515	-1.828887	3.371482	0.003283	0.711454
-16.618477	-1.895828	3.381478	0.003212	0.711455
-16.724497	-1.875552	3.391475	0.003232	0.711458
-15.995620	-1.897656	3.401472	0.003096	0.711673
-16.143176	-1.827216	3.411469	0.003124	0.711762
-15.899507	-1.870818	3.421466	0.003078	0.711761
-15.886368	-1.813051	3.431462	0.003076	0.711881
-15.101826	-1.846650	3.441459	0.002930	0.712093
-15.070519	-1.851510	3.451456	0.002924	0.712095
-14.968837	-1.872439	3.461453	0.002905	0.712089
-14.282989	-1.847774	3.471450	0.002777	0.712382
-14.043029	-1.889850	3.481446	0.002732	0.712383
-14.052737	-1.885165	3.491443	0.002734	0.712389
-13.851289	-1.835309	3.501440	0.002696	0.712560
-13.217618	-1.872728	3.511437	0.002578	0.712711
-13.247338	-1.868911	3.521434	0.002584	0.712708
-13.188053	-1.878794	3.531430	0.002573	0.712709
-12.527997	-1.849512	3.541427	0.002450	0.713002
-12.239487	-1.888651	3.551424	0.002396	0.713026
-12.205830	-1.895459	3.561421	0.002390	0.713025
-12.034717	-1.889489	3.571418	0.002358	0.713098
-11.275850	-1.891437	3.581414	0.002216	0.713363
-11.017093	-1.937369	3.591411	0.002168	0.713363
-11.374372	-1.872835	3.601408	0.002235	0.713365
-11.299466	-1.811861	3.611405	0.002220	0.713513
-10.569961	-1.871627	3.621402	0.002085	0.713653
-10.802764	-1.829154	3.631398	0.002128	0.713655
-10.523311	-1.829399	3.641395	0.002076	0.713754
-9.581969	-1.886454	3.651392	0.001900	0.713974
-9.536786	-1.893822	3.661389	0.001892	0.713975
-9.092396	-1.973455	3.671386	0.001809	0.713974
-9.107140	-1.905684	3.681382	0.001812	0.714104
-8.297836	-1.960676	3.691379	0.001661	0.714281
-8.474541	-1.928866	3.701376	0.001694	0.714282
-8.299722	-1.961926	3.711373	0.001661	0.714278
-8.134066	-1.917845	3.721370	0.001630	0.714425
-7.356283	-1.963751	3.731366	0.001486	0.714609
-7.351138	-1.965008	3.741363	0.001485	0.714608
-7.259538	-1.980251	3.751360	0.001467	0.714611
-7.151122	-1.939716	3.761357	0.001447	0.714729
-6.305887	-2.000271	3.771354	0.001290	0.714908
-6.626409	-1.941581	3.781350	0.001349	0.714912
-6.456797	-1.971233	3.791347	0.001318	0.714913
-6.243812	-1.912076	3.801344	0.001278	0.715106
-5.587603	-1.965263	3.811341	0.001156	0.715232
-5.760649	-1.935407	3.821338	0.001188	0.715230
-5.518336	-1.977418	3.831334	0.001143	0.715233
-4.774520	-1.958350	3.841331	0.001004	0.715533
-4.762897	-1.953273	3.851328	0.001002	0.715548
-4.800964	-1.948055	3.861325	0.001009	0.715545
-4.643048	-1.930998	3.871322	0.000979	0.715635
-3.773892	-1.959287	3.881318	0.000817	0.715885
-3.345505	-2.035231	3.891315	0.000738	0.715886
-3.798040	-1.955116	3.901312	0.000822	0.715885
-3.529012	-1.954556	3.911309	0.000772	0.715982
-3.063476	-1.960471	3.921306	0.000685	0.716134
-2.928197	-1.985897	3.931302	0.000660	0.716132
-3.037638	-1.960076	3.941299	0.000680	0.716145
-2.377013	-1.924557	3.951296	0.000557	0.716448
-2.141835	-1.967226	3.961293	0.000513	0.716447
-2.100895	-1.973044	3.971290	0.000505	0.716450
-1.790895	-1.932959	3.981286	0.000448	0.716639
-1.281765	-1.963266	3.991283	0.000353	0.716758
-1.398558	-1.943356	4.001280	0.000374	0.716757
-1.237566	-1.929727	4.011277	0.000344	0.716840
-0.912207	-1.864393	4.021274	0.000284	0.717084
-1.053912	-1.837835	4.031270	0.000310	0.717087
-0.862095	-1.818572	4.041267	0.000274	0.717193
-0.776833	-1.736930	4.051264	0.000258	0.717385
-0.845858	-1.726597	4.061261	0.000271	0.717381
-0.641912	-1.611154	4.071258	0.000233	0.717681
-0.536302	-1.616705	4.081254	0.000213	0.717707
-0.559742	-1.497911	4.091251	0.000217	0.717934
-0.523657	-1.461487	4.101248	0.000210	0.718019
-0.533457	-1.325129	4.111245	0.000212	0.718285
-0.627105	-1.262688	4.121242	0.000229	0.718375
-0.509286	-1.149547	4.131238	0.000207	0.718640
-0.399804	-1.089880	4.141235	0.000187	0.718797
-0.395796	-1.008282	4.151232	0.000186	0.718959
-0.235147	-0.883599	4.161229	0.000156	0.719262
-0.225525	-0.794227	4.171226	0.000154	0.719441
-0.242011	-0.684918	4.181222	0.000157	0.719651
-0.195224	-0.568365	4.191219	0.000148	0.719898
-0.076625	-0.443133	4.201216	0.000126	0.720186
-0.117451	-0.312710	4.211213	0.000133	0.720429
-0.184626	-0.167310	4.221210	0.000146	0.720691
-0.056876	-0.057089	4.231206	0.000122	0.720953
-0.042487	0.062799	4.241203	0.000119	0.721194
0.000000	0.235020	4.251200	0.000111	0.721548

0.087659	0.846042	4.256205	0.000094	0.722779
0.211878	2.086975	4.261210	0.000070	0.725254
0.428181	3.910455	4.266214	0.000029	0.728886
0.618228	6.283002	4.271219	-0.000008	0.733554
0.963157	9.134511	4.276224	-0.000075	0.739166
1.269957	12.485581	4.281229	-0.000134	0.745673
1.609878	16.277668	4.286234	-0.000200	0.752965
2.060671	20.456556	4.291238	-0.000286	0.760946
2.445413	25.044172	4.296243	-0.000361	0.769576
3.045637	29.967413	4.301248	-0.000476	0.778791
3.496064	35.264502	4.306253	-0.000563	0.788524
4.059453	40.853796	4.311258	-0.000672	0.798691
4.448199	46.788218	4.316262	-0.000748	0.809282
4.946430	52.978107	4.321267	-0.000845	0.820211
5.746289	59.391781	4.326272	-0.000998	0.831469
6.410385	66.062727	4.331277	-0.001126	0.842969
6.798635	72.995692	4.336282	-0.001203	0.854667
7.971473	80.004371	4.341286	-0.001426	0.866558
8.753368	87.279415	4.346291	-0.001576	0.878606
9.502286	94.728386	4.351296	-0.001721	0.890758
10.957222	102.231819	4.356301	-0.001997	0.903026
11.833381	109.986876	4.361306	-0.002165	0.915362
12.693193	117.863530	4.366310	-0.002330	0.927714
13.411238	125.890222	4.371315	-0.002469	0.940093
14.102686	134.024046	4.376320	-0.002603	0.952463
14.683091	142.265326	4.381325	-0.002717	0.964803
15.505320	150.544432	4.386330	-0.002875	0.977104
16.310733	158.914563	4.391334	-0.003031	0.989377
16.936355	167.364822	4.396339	-0.003153	1.001568
17.643112	175.836716	4.401344	-0.003290	1.013662
18.674175	184.298428	4.406349	-0.003487	1.025677
19.614373	192.808292	4.411354	-0.003668	1.037597
20.058883	201.428796	4.416358	-0.003756	1.049414
20.845775	210.010798	4.421363	-0.003909	1.061127
21.829907	218.592179	4.426368	-0.004097	1.072756
22.472846	227.234032	4.431373	-0.004223	1.084262
22.909269	235.923994	4.436378	-0.004310	1.095662
23.961782	244.506567	4.441382	-0.004511	1.106944
24.636917	253.167526	4.446387	-0.004643	1.118128
25.392143	261.804601	4.451392	-0.004789	1.129188
26.088892	270.458221	4.456397	-0.004924	1.140148
26.481289	279.161934	4.461402	-0.005003	1.151002
27.379544	287.767478	4.466406	-0.005176	1.161739
28.501572	296.317627	4.471411	-0.005391	1.172357
29.165533	304.935799	4.476416	-0.005520	1.182867
30.002069	313.537996	4.481421	-0.005681	1.193300
30.368262	322.175441	4.486426	-0.005755	1.203589
30.923325	330.790205	4.491430	-0.005864	1.213802
31.570211	339.358948	4.496435	-0.005990	1.223894
32.017926	347.970209	4.501440	-0.006079	1.233914
32.549898	356.517811	4.506445	-0.006184	1.243796
33.284623	365.024039	4.511450	-0.006326	1.253592
33.948959	373.533168	4.516454	-0.006456	1.263301
34.426567	382.071067	4.521459	-0.006550	1.272934
34.921099	390.568175	4.526464	-0.006648	1.282451
35.480688	399.065959	4.531469	-0.006758	1.291911
35.912296	407.550320	4.536474	-0.006843	1.301264
36.432754	416.087527	4.541478	-0.006946	1.310624
37.002416	424.579076	4.546483	-0.007058	1.319876
37.434049	433.002075	4.551488	-0.007143	1.328966
38.285689	441.371232	4.556493	-0.007308	1.338012
38.934604	449.742812	4.561498	-0.007434	1.346963
39.679719	458.116551	4.566502	-0.007578	1.355874
40.021403	466.527437	4.571507	-0.007647	1.364695
40.639781	474.901634	4.576512	-0.007768	1.373469
41.014352	483.308531	4.581517	-0.007843	1.382179
41.255978	491.722107	4.586522	-0.007894	1.390819
41.802112	500.076609	4.591526	-0.008001	1.399397
42.321390	508.405512	4.596531	-0.008103	1.407891
42.752172	516.758233	4.601536	-0.008189	1.416344
43.264038	525.089307	4.606541	-0.008289	1.424739
44.026133	533.377879	4.611546	-0.008437	1.433082
44.319755	541.726273	4.616550	-0.008497	1.441360
44.815834	550.032814	4.621555	-0.008595	1.449583
45.642105	558.287696	4.626560	-0.008754	1.457761
46.026927	566.611756	4.631565	-0.008831	1.465890
46.117467	575.014330	4.636570	-0.008853	1.474003
46.769079	583.260129	4.641574	-0.008980	1.482010
47.243248	591.527787	4.646579	-0.009074	1.489966
47.485138	599.834391	4.651584	-0.009124	1.497881
48.078745	608.074990	4.656589	-0.009240	1.505747
48.472786	616.356016	4.661594	-0.009319	1.513578
49.096334	624.577257	4.666598	-0.009441	1.521348
49.493287	632.845034	4.671603	-0.009520	1.529088
49.715584	641.139265	4.676608	-0.009567	1.536786
50.021970	649.403079	4.681613	-0.009629	1.544431
50.715855	657.619162	4.686618	-0.009764	1.552052
51.200902	665.851547	4.691622	-0.009860	1.559619
51.679674	674.064616	4.696627	-0.009954	1.567131
52.077154	682.308810	4.701632	-0.010034	1.574623
52.615403	690.519898	4.706637	-0.010139	1.582071
52.859350	698.764682	4.711642	-0.010190	1.589471
53.427858	706.984952	4.716646	-0.010301	1.596861
53.842663	715.193394	4.721651	-0.010384	1.604185
54.179939	723.425679	4.726656	-0.010452	1.611485
54.720566	731.636395	4.731661	-0.010558	1.618762
54.905785	739.869201	4.736666	-0.010598	1.625976
55.317694	748.138780	4.741670	-0.010680	1.633221
56.165741	756.253590	4.746675	-0.010843	1.640361
56.520649	764.442681	4.751680	-0.010915	1.647465
56.996112	772.664596	4.756685	-0.011009	1.654584
57.348251	780.838081	4.761690	-0.011080	1.661614
57.589131	789.066485	4.766694	-0.011130	1.668645
57.948180	797.264438	4.771699	-0.011202	1.675638
58.222821	805.436073	4.776704	-0.011259	1.682567
58.915894	813.581112	4.781709	-0.011393	1.689501
59.196866	821.779890	4.786714	-0.011451	1.696398
59.378434	829.989387	4.791718	-0.011490	1.703262
59.801953	838.171477	4.796723	-0.011574	1.710107
60.162773	846.350150	4.801728	-0.011647	1.716914
60.689651	854.487327	4.806733	-0.011750	1.723681
61.176641	862.624033	4.811738	-0.011846	1.730416
61.595822	870.808014	4.816742	-0.011930	1.737155
61.946783	878.973028	4.821747	-0.012000	1.743843
62.328632	887.138708	4.826752	-0.012077	1.750511
62.762675	895.317713	4.831757	-0.012163	1.757170
62.776193	903.510233	4.836762	-0.012171	1.763762
62.998840	911.684081	4.841766	-0.012218	1.770340
63.440980	919.832487	4.846771	-0.012305	1.776901
63.584443	928.000502	4.851776	-0.012337	1.783417
64.041477	936.158168	4.856781	-0.012428	1.789939
64.325151	944.343834	4.861786	-0.012486	1.796438
64.822468	952.452039	4.866790	-0.012584	1.802878
65.353242	960.544681	4.871795	-0.012688	1.809288
65.682256	968.697318	4.876800	-0.012755	1.815697
66.044440	976.841650	4.881805	-0.012827	1.822081
66.372669	984.979031	4.886810	-0.012894	1.828433
66.566325	993.162923	4.891814	-0.012935	1.834783
66.881285	1001.286918	4.896819	-0.012999	1.841080
67.176123	1009.422991	4.901824	-0.013060	1.847361
67.707586	1017.554468	4.906829	-0.013164	1.853646
68.093720	1025.673152	4.911834	-0.013241	1.859882
68.516432	1033.807086	4.916838	-0.013325	1.866113
68.653436	1042.011005	4.921843	-0.013356	1.872343
69.283917	1050.089908	4.926848	-0.013479	1.878515
69.613432	1058.207939	4.931853	-0.013545	1.884662
70.011885	1066.328760	4.936858	-0.013625	1.890799
70.337660	1074.463543	4.941862	-0.013691	1.896917
70.538915	1082.598477	4.946867	-0.013734	1.903002
71.063794	1090.687473	4.951872	-0.013837	1.909070
71.404707	1098.840449	4.956877	-0.013906	1.915145
71.626831	1106.952225	4.961882	-0.013952	1.921157
71.905982	1115.079112	4.966886	-0.014010	1.927168
72.233211	1123.217787	4.971891	-0.014076	1.933174
72.709848	1131.313623	4.976896	-0.014170	1.939146
73.184988	1139.406984	4.981901	-0.014264	1.945098
73.465777	1147.570875	4.986906	-0.014321	1.951062
73.761381	1155.719812	4.991910	-0.014382	1.956998
74.111463	1163.798387	4.996915	-0.014452	1.962871
74.629809	1171.878923	5.001920	-0.014554	1.968747
74.986082	1180.003468	5.006925	-0.014626	1.974618
75.246778	1188.111085	5.011930	-0.014679	1.980450
75.609972	1196.200636	5.016934	-0.014752	1.986263
76.060905	1204.324004	5.021939	-0.014842	1.992092
76.197618	1212.453686	5.026944	-0.014872	1.997875
76.634718	1220.537753	5.031949	-0.014959	2.003641
76.840630	1228.644283	5.036954	-0.015003	2.009381
77.148950	1236.768146	5.041958	-0.015066	2.015129
77.589420	1244.849152	5.046963	-0.015153	2.020843
77.909284	1252.947517	5.051968	-0.015218	2.026541
78.378458	1261.081689	5.056973	-0.015310	2.032263
78.549878	1269.190637	5.061978	-0.015348	2.037921
78.703446	1277.298985	5.066982	-0.015382	2.043560
79.095765	1285.394610	5.071987	-0.015460	2.049200
79.092083	1293.540774	5.076992	-0.015465	2.054819
79.442886	1301.617147	5.081997	-0.015535	2.060411
79.745764	1309.693825	5.087002	-0.015597	2.065982
79.948676	1317.817437	5.092006	-0.015640	2.071561
80.191784	1325.927487	5.097011	-0.015691	2.077119
80.559456	1333.980240	5.102016	-0.015764	2.082636
80.829754	1342.091605	5.107021	-0.015820	2.088168
81.136159	1350.189913	5.112026	-0.015882	2.093680
81.628074	1358.252592	5.117030	-0.015979	2.099172
82.208299	1366.313086	5.122035	-0.016093	2.104656
82.365002	1374.435371	5.127040	-0.016127	2.110127
82.771745	1382.594096	5.132045	-0.016208	2.115631
83.220190	1390.623347	5.137050	-0.016297	2.121039
83.259215	1398.736399	5.142054	-0.016310	2.126450
83.406878	1406.855243	5.147059	-0.016342	2.131861
83.628523	1414.926229	5.152064	-0.016389	2.137234
83.825475	1423.012270	5.157069	-0.016431	2.142600
83.757657	1431.127297	5.162074	-0.016424	2.147948
84.001060	1439.227970	5.167078	-0.016474	2.153302
84.315318	1447.296265	5.172083	-0.016538	2.158628
84.643476	1455.345281	5.177088	-0.016604	2.163929
85.294828	1463.385722	5.182093	-0.016731	2.169242
85.620007	1471.483181	5.187098	-0.016797	2.174548
86.038984	1479.540948	5.192102	-0.016880	2.179825
86.302352	1487.637263	5.197107	-0.016934	2.185099
86.642717	1495.733745	5.202112	-0.017003	2.190368
87.030969	1503.845876	5.207117	-0.017081	2.195638
87.172906	1511.916704	5.212122	-0.017113	2.200847
87.774740	1519.946512	5.217126	-0.017230	2.206059
87.838773	1528.078113	5.222131	-0.017247	2.211275
88.114596	1536.167640	5.227136	-0.017304	2.216471
88.202261	1544.272654	5.232141	-0.017325	2.221647
88.381748	1552.339308	5.237146	-0.017364	2.226795
88.659111	1560.422878	5.242150	-0.017421	2.231951
88.833091	1568.520815	5.247155	-0.017459	2.237095
89.209068	1576.540054	5.252160	-0.017534	2.242195
89.407072	1584.641581	5.257165	-0.017576	2.247320
89.666019	1592.719225	5.262170	-0.017630	2.252423
90.052101	1600.783753	5.267174	-0.017707	2.257518
90.382119	1608.864590	5.272179	-0.017774	2.262606
90.671222	1616.934266	5.277184	-0.017833	2.267672
90.864594	1625.100154	5.282189	-0.017874	2.272779
90.902284	1633.171908	5.287194	-0.017886	2.277802
91.024779	1641.224620	5.292198	-0.017915	2.282809
91.393784	1649.259594	5.297203	-0.017989	2.287816
91.572105	1657.333645	5.302208	-0.018027	2.292819
91.930369	1665.396662	5.307213	-0.018099	2.297820
92.265379	1673.447419	5.312218	-0.018167	2.302801
92.651181	1681.505573	5.317222	-0.018244	2.307779
93.093507	1689.582085	5.322227	-0.018331	2.312763
93.216362	1697.655336	5.327232	-0.018360	2.317707
93.469088	1705.727160	5.332237	-0.018412	2.322651
93.679048	1713.790614	5.337242	-0.018456	2.327575
94.057847	1721.864261	5.342246	-0.018532	2.332509
94.128133	1729.964476	5.347251	-0.018551	2.337423
94.293897	1738.020249	5.352256	-0.018587	2.342308
94.798252	1746.071135	5.357261	-0.018686	2.347207
94.907696	1754.166197	5.362266	-0.018712	2.352091
95.034078	1762.257414	5.367270	-0.018740	2.356963
95.392483	1770.282030	5.372275	-0.018812	2.361804
95.761002	1778.319388	5.377280	-0.018886	2.366644
95.822032	1786.427407	5.382285	-0.018903	2.371491
96.254761	1794.466969	5.387290	-0.018989	2.376317
96.204189	1802.549952	5.392294	-0.018985	2.381121
96.430261	1810.622687	5.397299	-0.019032	2.385930
96.726922	1818.666287	5.402304	-0.019093	2.390719
97.212517	1826.732953	5.407309	-0.019188	2.395526
97.226646	1834.807032	5.412314	-0.019196	2.400291
97.508653	1842.858827	5.417318	-0.019254	2.405054
97.552467	1850.947305	5.422323	-0.019268	2.409811
97.887264	1859.006484	5.427328	-0.019335	2.414564
97.886113	1867.110591	5.432333	-0.019340	2.419307
98.381268	1875.116190	5.437338	-0.019438	2.424022
98.674592	1883.179412	5.442342	-0.019498	2.428746
99.048388	1891.310740	5.447347	-0.019573	2.433507
99.141763	1899.358015	5.452352	-0.019595	2.438187
99.624910	1907.371654	5.457357	-0.019690	2.442869
100.125407	1915.383584	5.462362	-0.019789	2.447543
101.094245	1923.385929	5.467366	-0.019975	2.452237
101.514161	1931.450449	5.472371	-0.020058	2.456916
101.783532	1939.498990	5.477376	-0.020113	2.461566
102.036514	1947.602360	5.482381	-0.020166	2.466238
102.089303	1955.705401	5.487386	-0.020181	2.470885
102.537514	1963.752818	5.492390	-0.020270	2.475521
102.920204	1971.798141	5.497395	-0.020346	2.480142
102.894597	1979.862961	5.502400	-0.020347	2.484736
103.254217	1987.929536	5.507405	-0.020419	2.489350
103.300768	1996.029576	5.512410	-0.020433	2.493952
103.465252	2004.086349	5.517414	-0.020469	2.498530
103.759549	2012.140970	5.522419	-0.020529	2.503107
103.941060	2020.196292	5.527424	-0.020568	2.507668
104.400063	2028.268659	5.532429	-0.020659	2.512251
104.450708	2036.338565	5.537434	-0.020674	2.516794
104.892431	2044.357035	5.542438	-0.020761	2.521328
104.941144	2052.421358	5.547443	-0.020775	2.525852
105.023211	2060.492280	5.552448	-0.020796	2.530373
105.407861	2068.548268	5.557453	-0.020873	2.534900
105.708002	2076.578118	5.562458	-0.020934	2.539397
105.911969	2084.607978	5.567462	-0.020977	2.543880
106.019328	2092.707457	5.572467	-0.021003	2.548387
106.116102	2100.786631	5.577472	-0.021026	2.552874
106.478063	2108.818803	5.582477	-0.021099	2.557346
106.759978	2116.831291	5.587482	-0.021156	2.561793
106.910919	2124.891150	5.592486	-0.021190	2.566250
107.219509	2132.965936	5.597491	-0.021253	2.570718
107.291023	2141.033400	5.602496	-0.021271	2.575157
107.751391	2149.048830	5.607501	-0.021362	2.579588
108.098319	2157.088872	5.612506	-0.021432	2.584016
108.360478	2165.145273	5.617510	-0.021486	2.588440
108.815624	2173.344568	5.622515	-0.021576	2.592947
109.283964	2181.359815	5.627520	-0.021669	2.597347
109.438927	2189.395041	5.632525	-0.021703	2.601729
109.572547	2197.414935	5.637530	-0.021733	2.606094
109.728643	2205.465447	5.642534	-0.021767	2.610469
110.019412	2213.534483	5.647539	-0.021827	2.614857
110.177228	2221.542390	5.652544	-0.021861	2.619195
110.355444	2229.588661	5.657549	-0.021900	2.623548
110.522127	2237.613867	5.662554	-0.021936	2.627881
110.621723	2245.697030	5.667558	-0.021960	2.632234
110.907114	2253.766372	5.672563	-0.022018	2.636585
111.098083	2261.769017	5.677568	-0.022059	2.640886
111.316609	2269.814147	5.682573	-0.022105	2.645205
111.509764	2277.854619	5.687578	-0.022146	2.649513
111.938333	2285.911393	5.692582	-0.022232	2.653838
112.112502	2293.972486	5.697587	-0.022269	2.658141
112.199759	2302.008581	5.702592	-0.022291	2.662419
112.522425	2310.062516	5.707597	-0.022356	2.666714
112.844270	2318.120891	5.712602	-0.022421	2.671004
112.827439	2326.230623	5.717606	-0.022424	2.675293
113.225550	2334.209555	5.722611	-0.022503	2.679533
113.464719	2342.232467	5.727616	-0.022553	2.683779
113.922999	2350.262505	5.732621	-0.022643	2.688036
113.870894	2358.360634	5.737626	-0.022639	2.692289
114.041157	2366.395923	5.742630	-0.022676	2.696517
114.569088	2374.414002	5.747635	-0.022779	2.700752
114.603620	2382.467238	5.752640	-0.022791	2.704967
114.770970	2390.515337	5.757645	-0.022828	2.709181
115.122778	2398.598313	5.762650	-0.022898	2.713419
115.279094	2406.643709	5.767654	-0.022933	2.717618
115.447323	2414.699022	5.772659	-0.022969	2.721817
115.751669	2422.715747	5.777664	-0.023031	2.725997
115.976421	2430.767089	5.782669	-0.023078	2.730184
116.061123	2438.842735	5.787674	-0.023100	2.734368
116.288290	2446.870377	5.792678	-0.023147	2.738530
116.774150	2454.898512	5.797683	-0.023243	2.742702
116.863610	2462.965997	5.802688	-0.023265	2.746863
117.181660	2471.045527	5.807693	-0.023329	2.751038
117.329408	2479.155152	5.812698	-0.023362	2.755212
117.457498	2487.162496	5.817702	-0.023391	2.759326
117.814812	2495.180582	5.822707	-0.023463	2.763453
118.202487	2503.162082	5.827712	-0.023540	2.767557
118.484825	2511.238979	5.832717	-0.023598	2.771697
118.740133	2519.280405	5.837722	-0.023651	2.775811
118.844932	2527.291926	5.842726	-0.023676	2.779895
118.933086	2535.331986	5.847731	-0.023698	2.783986
119.240208	2543.367711	5.852736	-0.023760	2.788082
119.550470	2551.426783	5.857741	-0.023823	2.792184
119.817637	2559.474478	5.862746	-0.023878	2.796272
120.056425	2567.508945	5.867750	-0.023928	2.800345
120.380990	2575.519954	5.872755	-0.023994	2.804406
120.506151	2583.563270	5.877760	-0.024022	2.808465
120.817579	2591.637234	5.882765	-0.024085	2.812544
120.873884	2599.712607	5.887770	-0.024101	2.816604
120.898930	2607.751555	5.892774	-0.024111	2.820638
121.424629	2615.744707	5.897779	-0.024214	2.824671
121.488735	2623.814215	5.902784	-0.024231	2.828711
121.718940	2631.898243	5.907789	-0.024280	2.832761
122.041652	2639.929563	5.912794	-0.024345	2.836785
122.304929	2647.935944	5.917798	-0.024399	2.840787
122.644787	2655.956381	5.922803	-0.024468	2.844795
122.634177	2663.995328	5.927808	-0.024471	2.848786
123.059012	2672.067479	5.932813	-0.024555	2.852813
123.185615	2680.091584	5.937818	-0.024584	2.856794
123.403855	2688.121049	5.942822	-0.024630	2.860776
123.871286	2696.141376	5.947827	-0.024723	2.864763
124.207442	2704.175217	5.952832	-0.024790	2.868743
124.188739	2712.281144	5.957837	-0.024792	2.872734
124.575674	2720.286849	5.962842	-0.024870	2.876692
124.624338	2728.337154	5.967846	-0.024884	2.880647
124.933474	2736.362488	5.972851	-0.024947	2.884600
124.909174	2744.409349	5.977856	-0.024947	2.888539
125.306750	2752.462446	5.982861	-0.025027	2.892499
125.698631	2760.496090	5.987866	-0.025105	2.896444
125.876527	2768.528740	5.992870	-0.025143	2.900371
126.099553	2776.571881	5.997875	-0.025190	2.904300
126.397787	2784.590761	6.002880	-0.025251	2.908217
126.642614	2792.707547	6.007885	-0.025302	2.912172
126.906483	2800.776737	6.012890	-0.025356	2.916100
127.086083	2808.756571	6.017894	-0.025395	2.919975
127.402835	2816.765655	6.022899	-0.025459	2.923867
127.500335	2824.803758	6.027904	-0.025483	2.927755
127.691323	2832.861173	6.032909	-0.025524	2.931653
128.035419	2840.905593	6.037914	-0.025593	2.935547
128.122207	2848.901894	6.042918	-0.025614	2.939399
128.328028	2856.950414	6.047923	-0.025658	2.943277
128.449693	2864.985596	6.052928	-0.025686	2.947140
128.738940	2873.049751	6.057933	-0.025745	2.951020
128.613898	2881.121805	6.062938	-0.025727	2.954877
128.877131	2889.121945	6.067942	-0.025781	2.958715
129.242773	2897.148423	6.072947	-0.025855	2.962566
129.325839	2905.175292	6.077952	-0.025875	2.966397
129.610614	2913.229658	6.082957	-0.025934	2.970247
129.519681	2921.313188	6.087962	-0.025922	2.974086
129.741838	2929.316427	6.092966	-0.025969	2.977898
129.970922	2937.353677	6.097971	-0.026017	2.981722
130.096038	2945.368920	6.102976	-0.026045	2.985526
130.390275	2953.410814	6.107981	-0.026105	2.989345
130.418861	2961.523743	6.112986	-0.026116	2.993180
130.872060	2969.489580	6.117990	-0.026205	2.996961
131.029758	2977.529445	6.122995	-0.026240	3.000758
131.072327	2985.513417	6.128000	-0.026253	3.004519
131.419322	2993.553101	6.133005	-0.026323	3.008315
131.599872	3001.605994	6.138010	-0.026362	3.012105
131.787053	3009.665770	6.143014	-0.026402	3.015894
131.928058	3017.691928	6.148019	-0.026434	3.019659
132.388620	3025.661379	6.153024	-0.026525	3.023409
132.504890	3033.729732	6.158029	-0.026552	3.027184
132.646758	3041.808905	6.163034	-0.026583	3.030961
132.858674	3049.841343	6.168038	-0.026628	3.034714
133.246040	3057.873688	6.173043	-0.026705	3.038471
133.241130	3065.901037	6.178048	-0.026710	3.042202
133.746188	3073.896958	6.183053	-0.026809	3.045938
134.038296	3081.937068	6.188058	-0.026869	3.049681
134.178103	3089.998851	6.193062	-0.026900	3.053421
134.369626	3098.067983	6.198067	-0.026941	3.057162
134.648722	3106.056976	6.203072	-0.026998	3.060866
134.786255	3114.102114	6.208077	-0.027029	3.064585
135.008479	3122.157258	6.213082	-0.027076	3.068307
135.043033	3130.252990	6.218086	-0.027087	3.072035
135.263082	3138.341731	6.223091	-0.027134	3.075764
135.092405	3146.319562	6.228096	-0.027107	3.079419
135.386616	3154.320255	6.233101	-0.027167	3.083103
135.657456	3162.328946	6.238106	-0.027223	3.086784
135.879993	3170.335837	6.243110	-0.027270	3.090457
135.947820	3178.404893	6.248115	-0.027288	3.094148
136.155414	3186.425754	6.253120	-0.027331	3.097818
136.384600	3194.467775	6.258125	-0.027379	3.101495
136.479727	3202.484198	6.263130	-0.027402	3.105150
136.845336	3210.494040	6.268134	-0.027476	3.108809
137.086607	3218.556190	6.273139	-0.027526	3.112483
137.187648	3226.597223	6.278144	-0.027550	3.116136
137.315781	3234.614726	6.283149	-0.027579	3.119775
137.718511	3242.602663	6.288154	-0.027659	3.123409
137.872215	3250.649666	6.293158	-0.027693	3.127054
137.950695	3258.744020	6.298163	-0.027713	3.130713
138.147260	3266.757286	6.303168	-0.027755	3.134337
138.512107	3274.775138	6.308173	-0.027828	3.137965
138.707611	3282.792041	6.313178	-0.027870	3.141582
138.823905	3290.816332	6.318182	-0.027897	3.145194
139.218726	3298.878294	6.323187	-0.027976	3.148831
139.360529	3306.934811	6.328192	-0.028007	3.152451
139.428929	3314.993879	6.333197	-0.028025	3.156064
139.844421	3322.976771	6.338202	-0.028108	3.159654
139.979529	3330.973831	6.343206	-0.028138	3.163234
140.109972	3339.046253	6.348211	-0.028168	3.166843
140.311780	3347.039789	6.353216	-0.028211	3.170416
140.552226	3355.120775	6.358221	-0.028261	3.174026
140.843009	3363.124087	6.363226	-0.028320	3.177599
141.206959	3371.143580	6.368230	-0.028393	3.181178
141.887802	3379.126394	6.373235	-0.028525	3.184751
142.155802	3387.186951	6.378240	-0.028580	3.188336
142.372509	3395.253867	6.383245	-0.028626	3.191918
142.456621	3403.333428	6.388250	-0.028647	3.195496
142.761150	3411.286590	6.393254	-0.028709	3.199023
142.955352	3419.346216	6.398259	-0.028750	3.202589
142.927924	3427.396266	6.403264	-0.028751	3.206137
143.346857	3435.406608	6.408269	-0.028834	3.209682
143.361643	3443.469154	6.413274	-0.028842	3.213230
143.351102	3451.499649	6.418278	-0.028845	3.216758
143.749336	3459.488426	6.423283	-0.028925	3.220281
143.688053	3467.521441	6.428288	-0.028918	3.223801
143.946436	3475.567508	6.433293	-0.028972	3.227336
144.218159	3483.623427	6.438298	-0.029028	3.230872
144.252379	3491.713319	6.443302	-0.029039	3.234409
144.578684	3499.706199	6.448307	-0.029105	3.237911
144.771634	3507.689483	6.453312	-0.029147	3.241400
145.010402	3515.710928	6.458317	-0.029196	3.244904
145.067179	3523.748664	6.463322	-0.029212	3.248404
145.236353	3531.758141	6.468326	-0.029249	3.251892
145.557837	3539.814799	6.473331	-0.029314	3.255403
145.708883	3547.820361	6.478336	-0.029347	3.258881
145.797602	3555.867668	6.483341	-0.029369	3.262371
146.040114	3563.904519	6.488346	-0.029420	3.265859
146.019266	3571.908384	6.493350	-0.029421	3.269319
146.386024	3579.990284	6.498355	-0.029495	3.272823
146.358289	3588.030737	6.503360	-0.029495	3.276291
146.606947	3596.022008	6.508365	-0.029546	3.279745
146.870105	3604.024870	6.513370	-0.029600	3.283200
146.903366	3612.044718	6.518374	-0.029612	3.286650
147.234435	3620.091253	6.523379	-0.029679	3.290120
147.425320	3628.129215	6.528384	-0.029720	3.293576
147.736465	3636.160554	6.533389	-0.029783	3.297031
147.936560	3644.190726	6.538394	-0.029825	3.300478
148.106244	3652.193412	6.543398	-0.029862	3.303907
148.297408	3660.241328	6.548403	-0.029903	3.307354
148.253595	3668.294498	6.553408	-0.029900	3.310790
148.488793	3676.362747	6.558413	-0.029949	3.314239
148.617144	3684.366862	6.563418	-0.029978	3.317654
148.524814	3692.392926	6.568422	-0.029967	3.321066
148.904731	3700.364247	6.573427	-0.030042	3.324469
149.150902	3708.351281	6.578432	-0.030094	3.327870
149.334952	3716.452201	6.583437	-0.030133	3.331314
149.588383	3724.483289	6.588442	-0.030186	3.334727
149.798333	3732.467510	6.593446	-0.030230	3.338115
150.095916	3740.507698	6.598451	-0.030291	3.341526
150.283379	3748.505211	6.603456	-0.030331	3.344912
150.462608	3756.553823	6.608461	-0.030369	3.348315
150.632600	3764.636706	6.613466	-0.030406	3.351730
150.731974	3772.667281	6.618470	-0.030430	3.355116
151.097303	3780.686055	6.623475	-0.030503	3.358503
151.366607	3788.669351	6.628480	-0.030559	3.361869
151.548028	3796.701801	6.633485	-0.030598	3.365248
151.746355	3804.750651	6.638490	-0.030640	3.368632
151.693996	3812.812723	6.643494	-0.030636	3.372009
152.077094	3820.847963	6.648499	-0.030712	3.375386
152.171317	3828.849550	6.653504	-0.030735	3.378736
152.519182	3836.857783	6.658509	-0.030805	3.382095
152.620794	3844.903984	6.663514	-0.030829	3.385457
152.878180	3852.924102	6.668518	-0.030882	3.388810
153.164700	3861.022570	6.673523	-0.030941	3.392194
153.472332	3869.065945	6.678528	-0.031004	3.395552
153.634489	3877.037228	6.683533	-0.031039	3.398871
153.648983	3885.055823	6.688538	-0.031047	3.402202
153.762511	3893.046918	6.693542	-0.031073	3.405522
154.017340	3901.075540	6.698547	-0.031126	3.408859
154.013826	3909.119302	6.703552	-0.031131	3.412189
154.155022	3917.169498	6.708557	-0.031162	3.415525
154.384803	3925.172692	6.713562	-0.031210	3.418840
154.519895	3933.177971	6.718566	-0.031241	3.422150
154.804253	3941.216638	6.723571	-0.031299	3.425476
154.733096	3949.234105	6.728576	-0.031291	3.428777
155.080968	3957.251480	6.733581	-0.031361	3.432090
155.338223	3965.305445	6.738586	-0.031414	3.435411
155.426777	3973.272388	6.743590	-0.031436	3.438687
155.788130	3981.322934	6.748595	-0.031508	3.442004
155.859151	3989.347870	6.753600	-0.031527	3.445298
156.052658	3997.388901	6.758605	-0.031568	3.448599
156.254594	4005.454605	6.763610	-0.031611	3.451907
156.204886	4013.488851	6.768614	-0.031607	3.455190
156.406630	4021.512034	6.773619	-0.031650	3.458475
156.926852	4029.498266	6.778624	-0.031752	3.461751
156.960799	4037.550375	6.783629	-0.031764	3.465036
157.066916	4045.604386	6.788634	-0.031789	3.468320
157.172610	4053.629282	6.793638	-0.031814	3.471589
157.567330	4061.682629	6.798643	-0.031892	3.474876
157.871620	4069.625620	6.803648	-0.031954	3.478113
158.010646	4077.670804	6.808653	-0.031985	3.481382
158.460781	4085.632837	6.813658	-0.032075	3.484625
158.600015	4093.678620	6.818662	-0.032106	3.487888
158.727943	4101.762228	6.823667	-0.032135	3.491163
158.844629	4109.767845	6.828672	-0.032162	3.494404
159.256584	4117.799660	6.833677	-0.032244	3.497661
159.285103	4125.845800	6.838682	-0.032254	3.500909
159.612718	4133.786327	6.843686	-0.032321	3.504120
159.840040	4141.866916	6.848691	-0.032368	3.507382
159.986106	4149.872936	6.853696	-0.032401	3.510608
160.221329	4157.945558	6.858701	-0.032450	3.513861
160.643569	4165.928188	6.863706	-0.032534	3.517081
160.572871	4173.922677	6.868710	-0.032526	3.520287
160.661614	4181.989355	6.873715	-0.032548	3.523523
160.969561	4190.010119	6.878720	-0.032610	3.526746
161.086479	4198.013105	6.883725	-0.032637	3.529952
161.266630	4206.101434	6.888730	-0.032676	3.533191
161.264867	4214.172739	6.893734	-0.032681	3.536415
161.477483	4222.139741	6.898739	-0.032726	3.539601
161.777415	4230.145047	6.903744	-0.032787	3.542802
162.135205	4238.147116	6.908749	-0.032859	3.546001
162.369039	4246.212173	6.913754	-0.032908	3.549218
162.579703	4254.284038	6.918758	-0.032952	3.552434
162.648919	4262.394310	6.923763	-0.032970	3.555658
162.662092	4270.322569	6.928768	-0.032978	3.558805
162.810614	4278.349421	6.933773	-0.033011	3.561993
163.038891	4286.340586	6.938778	-0.033059	3.565166
163.219474	4294.335399	6.943782	-0.033098	3.568336
163.521328	4302.409038	6.948787	-0.033159	3.571538
163.585799	4310.407896	6.953792	-0.033176	3.574700
163.727327	4318.434340	6.958797	-0.033208	3.577873
163.838146	4326.477349	6.963802	-0.033234	3.581049
164.042417	4334.444665	6.968806	-0.033277	3.584195
164.130457	4342.506052	6.973811	-0.033299	3.587371
164.172572	4350.522382	6.978816	-0.033312	3.590526
164.620968	4358.550612	6.983821	-0.033401	3.593694
164.959117	4366.587716	6.988826	-0.033469	3.596860
165.004604	4374.583828	6.993830	-0.033483	3.599998
165.384274	4382.584515	6.998835	-0.033558	3.603145
165.460838	4390.616425	7.003840	-0.033578	3.606293
165.543973	4398.615817	7.008845	-0.033599	3.609426
165.823976	4406.671323	7.013850	-0.033656	3.612583
165.920435	4414.715034	7.018854	-0.033679	3.615728
165.992742	4422.746699	7.023859	-0.033698	3.618865
166.245699	4430.741402	7.028864	-0.033750	3.621989
166.689251	4438.724122	7.033869	-0.033838	3.625112
166.946857	4446.786338	7.038874	-0.033892	3.628257
166.912397	4454.827904	7.043878	-0.033890	3.631384
167.187158	4462.887794	7.048883	-0.033947	3.634523
167.291729	4470.911910	7.053888	-0.033972	3.637641
167.258660	4478.915468	7.058893	-0.033971	3.640745
167.474644	4486.934422	7.063898	-0.034016	3.643859
167.573071	4494.947471	7.068902	-0.034040	3.646965
167.836289	4502.970607	7.073907	-0.034094	3.650076
167.955671	4511.003299	7.078912	-0.034122	3.653185
168.323315	4519.026737	7.083917	-0.034195	3.656294
168.392011	4527.057315	7.088922	-0.034213	3.659395
168.313957	4535.050446	7.093926	-0.034204	3.662475
168.753087	4543.080089	7.098931	-0.034291	3.665580
168.955827	4551.106751	7.103936	-0.034334	3.668675
168.965015	4559.163072	7.108941	-0.034341	3.671774
169.033245	4567.229560	7.113946	-0.034359	3.674876
169.351238	4575.186935	7.118950	-0.034423	3.677940
169.616135	4583.231979	7.123955	-0.034478	3.681033
169.553347	4591.178628	7.128960	-0.034472	3.684077
169.697733	4599.242025	7.133965	-0.034504	3.687169
170.049944	4607.291975	7.138970	-0.034575	3.690259
170.064731	4615.313110	7.143974	-0.034583	3.693326
170.262534	4623.365672	7.148979	-0.034625	3.696408
170.315716	4631.360081	7.153984	-0.034640	3.699461
170.595972	4639.342994	7.158989	-0.034697	3.702513
170.828449	4647.376718	7.163994	-0.034746	3.705580
171.008093	4655.385375	7.168998	-0.034785	3.708634
171.095013	4663.493750	7.174003	-0.034806	3.711721
171.209425	4671.557848	7.179008	-0.034833	3.714789
171.436045	4679.535920	7.184013	-0.034880	3.717825
171.539446	4687.531007	7.189018	-0.034905	3.720862
171.575562	4695.494982	7.194022	-0.034917	3.723883
171.927483	4703.534303	7.199027	-0.034987	3.726937
172.117417	4711.522222	7.204032	-0.035028	3.729966
172.195350	4719.570897	7.209037	-0.035048	3.733012
172.497385	4727.664067	7.214042	-0.035109	3.736078
172.611462	4735.595591	7.219046	-0.035136	3.739077
173.039132	4743.617278	7.224051	-0.035221	3.742114
173.007082	4751.633080	7.229056	-0.035220	3.745135
173.179614	4759.716348	7.234061	-0.035257	3.748184
173.363391	4767.771562	7.239066	-0.035297	3.751221
173.327600	4775.755685	7.244070	-0.035295	3.754223
173.834747	4783.779889	7.249075	-0.035395	3.757250
173.747196	4791.791774	7.254080	-0.035384	3.760257
173.968779	4799.786858	7.259085	-0.035431	3.763262
174.111776	4807.839075	7.264090	-0.035462	3.766284
174.381173	4815.833407	7.269094	-0.035518	3.769285
174.615951	4823.920621	7.274099	-0.035567	3.772317
174.477235	4831.943612	7.279104	-0.035546	3.775315
174.630781	4839.961078	7.284109	-0.035580	3.778314
174.900028	4848.020663	7.289114	-0.035636	3.781330
174.794401	4855.961196	7.294118	-0.035621	3.784290
175.098385	4864.006492	7.299123	-0.035683	3.787296
175.561855	4872.032018	7.304128	-0.035775	3.790296
175.728986	4880.082608	7.309133	-0.035811	3.793296
175.683498	4888.105252	7.314138	-0.035808	3.796279
175.888068	4896.065604	7.319142	-0.035851	3.799242
176.220196	4904.123988	7.324147	-0.035918	3.802242
176.651176	4912.071964	7.329152	-0.036004	3.805200
176.537124	4920.144189	7.334157	-0.035988	3.808190
176.854023	4928.185740	7.339162	-0.036052	3.811176
176.802910	4936.206230	7.344166	-0.036048	3.814144
177.334525	4944.227005	7.349171	-0.036152	3.817122
177.509261	4952.197174	7.354176	-0.036190	3.820071
177.558528	4960.179971	7.359181	-0.036204	3.823020
177.554947	4968.272716	7.364186	-0.036209	3.826007
177.693341	4976.255239	7.369190	-0.036240	3.828953
177.907568	4984.349853	7.374195	-0.036285	3.831940
177.785019	4992.341928	7.379200	-0.036267	3.834879
178.010105	5000.346710	7.384205	-0.036315	3.837829
178.458969	5008.402047	7.389210	-0.036403	3.840799
178.482257	5016.329607	7.394214	-0.036413	3.843711
178.686640	5024.414728	7.399219	-0.036456	3.846683
179.036295	5032.375440	7.404224	-0.036527	3.849609
179.233324	5040.439508	7.409229	-0.036569	3.852568
179.390701	5048.500127	7.414234	-0.036603	3.855523
179.523512	5056.487269	7.419238	-0.036633	3.858448
179.945830	5064.563679	7.424243	-0.036717	3.861409
180.038614	5072.497007	7.429248	-0.036740	3.864309
180.095470	5080.579477	7.434253	-0.036756	3.867261
180.208910	5088.644519	7.439258	-0.036782	3.870205
180.413933	5096.857313	7.444262	-0.036826	3.873202
180.419433	5104.866972	7.449267	-0.036832	3.876119
180.778937	5112.757165	7.454272	-0.036904	3.878998
180.843425	5120.717329	7.459277	-0.036921	3.881894
180.957080	5128.691152	7.464282	-0.036948	3.884794
181.102896	5136.738944	7.469286	-0.036980	3.887719
181.219793	5144.759111	7.474291	-0.037007	3.890631
181.340633	5152.772215	7.479296	-0.037035	3.893538
181.232983	5160.841357	7.484301	-0.037020	3.896459
181.706614	5168.797093	7.489306	-0.037113	3.899349
181.604839	5176.815844	7.494310	-0.037100	3.902247
181.813976	5184.833800	7.499315	-0.037144	3.905150
181.903484	5192.864901	7.504320	-0.037166	3.908052
182.256023	5200.884933	7.509325	-0.037237	3.910953
182.411536	5208.954153	7.514330	-0.037271	3.913867
182.492611	5216.939691	7.519334	-0.037291	3.916746
182.750340	5224.959392	7.524339	-0.037345	3.919639
182.778673	5232.972538	7.529344	-0.037355	3.922523
182.807058	5240.948172	7.534349	-0.037366	3.925391
182.978116	5249.003267	7.539354	-0.037403	3.928289
183.185110	5257.023437	7.544358	-0.037447	3.931172
183.406128	5265.074999	7.549363	-0.037493	3.934065
183.713301	5273.066429	7.554368	-0.037555	3.936936
183.808396	5281.065686	7.559373	-0.037578	3.939804
183.878698	5289.093858	7.564378	-0.037597	3.942679
183.887672	5297.117867	7.569382	-0.037604	3.945550
184.281030	5305.129665	7.574387	-0.037682	3.948421
184.573920	5313.152400	7.579392	-0.037742	3.951292
184.763415	5321.201905	7.584397	-0.037783	3.954168
185.040700	5329.244330	7.589402	-0.037839	3.957042
185.099125	5337.207830	7.594406	-0.037856	3.959881
185.515543	5345.207138	7.599411	-0.037938	3.962737
185.340769	5353.236452	7.604416	-0.037911	3.965592
185.586613	5361.219721	7.609421	-0.037962	3.968436
185.851032	5369.300211	7.614426	-0.038017	3.971312
185.653230	5377.288164	7.619430	-0.037985	3.974146
186.047950	5385.356666	7.624435	-0.038064	3.977016
186.043828	5393.334600	7.629440	-0.038068	3.979845
186.147687	5401.356331	7.634445	-0.038093	3.982689
186.346570	5409.388227	7.639450	-0.038135	3.985537
186.529394	5417.394050	7.644454	-0.038174	3.988373
186.630390	5425.455376	7.649459	-0.038199	3.991225
186.929993	5433.513351	7.654464	-0.038260	3.994077
187.244259	5441.540284	7.659469	-0.038323	3.996917
187.416509	5449.498135	7.664474	-0.038361	3.999728
187.477466	5457.509249	7.669478	-0.038377	4.002553
187.936785	5465.556732	7.674483	-0.038468	4.005396
188.045562	5473.584282	7.679488	-0.038494	4.008224
188.222860	5481.578080	7.684493	-0.038532	4.011040
188.251829	5489.667717	7.689498	-0.038543	4.013885
188.499837	5497.702677	7.694502	-0.038594	4.016712
188.253343	5505.691537	7.699507	-0.038553	4.019513
188.553715	5513.694632	7.704512	-0.038615	4.022325
188.872230	5521.675049	7.709517	-0.038679	4.025128
188.932809	5529.749133	7.714522	-0.038696	4.027958
188.768894	5537.745059	7.719526	-0.038670	4.030755
189.262237	5545.873253	7.724531	-0.038768	4.033606
189.484947	5553.886909	7.729536	-0.038814	4.036411
189.753711	5561.770173	7.734541	-0.038870	4.039170
189.761046	5569.835631	7.739546	-0.038876	4.041986
189.766192	5577.774337	7.744550	-0.038882	4.044756
190.030145	5585.819475	7.749555	-0.038937	4.047564
190.416709	5593.852588	7.754560	-0.039014	4.050369
190.445342	5601.888555	7.759565	-0.039025	4.053167
190.919489	5609.902464	7.764570	-0.039118	4.055962
190.760206	5617.862274	7.769574	-0.039094	4.058727
191.026698	5625.945520	7.774579	-0.039149	4.061540
191.141425	5633.934612	7.779584	-0.039175	4.064315
191.329081	5641.933425	7.784589	-0.039215	4.067093
191.571722	5649.956260	7.789594	-0.039266	4.069878
191.912057	5657.986130	7.794598	-0.039335	4.072665
192.138193	5666.016356	7.799603	-0.039382	4.075449
192.114144	5674.021642	7.804608	-0.039383	4.078218
192.546747	5682.018561	7.809613	-0.039469	4.080990
192.614426	5690.062789	7.814618	-0.039486	4.083770
192.789027	5698.067586	7.819622	-0.039524	4.086536
192.931660	5706.089107	7.824627	-0.039556	4.089306
193.169542	5714.127783	7.829632	-0.039606	4.092081
193.332862	5722.126000	7.834637	-0.039641	4.094840
193.589012	5730.185020	7.839642	-0.039694	4.097618
193.701639	5738.175322	7.844646	-0.039720	4.100369
193.758310	5746.175926	7.849651	-0.039736	4.103121
193.909991	5754.228270	7.854656	-0.039770	4.105891
194.143905	5762.225690	7.859661	-0.039819	4.108640
194.497108	5770.310493	7.864666	-0.039890	4.111419
194.304763	5778.348682	7.869670	-0.039859	4.114174
194.710198	5786.349668	7.874675	-0.039940	4.116921
194.894939	5794.286919	7.879680	-0.039979	4.119642
194.982687	5802.300631	7.884685	-0.040001	4.122386
195.164985	5810.351837	7.889690	-0.040040	4.125142
195.237731	5818.366858	7.894694	-0.040059	4.127882
195.320964	5826.420689	7.899699	-0.040080	4.130634
195.520704	5834.440008	7.904704	-0.040122	4.133374
195.767178	5842.494173	7.909709	-0.040173	4.136125
196.058946	5850.485298	7.914714	-0.040233	4.138852
195.994685	5858.497332	7.919718	-0.040226	4.141581
195.914646	5866.481252	7.924723	-0.040217	4.144298
196.205222	5874.539863	7.929728	-0.040276	4.147043
196.328866	5882.533585	7.934733	-0.040304	4.149763
196.479078	5890.597858	7.939738	-0.040338	4.152504
196.695425	5898.580604	7.944742	-0.040383	4.155217
196.848498	5906.658296	7.949747	-0.040417	4.157960
196.920963	5914.637333	7.954752	-0.040436	4.160666
196.873639	5922.600827	7.959757	-0.040432	4.163365
196.988306	5930.681995	7.964762	-0.040459	4.166103
197.070013	5938.658913	7.969766	-0.040479	4.168803
197.237530	5946.726800	7.974771	-0.040516	4.171534
197.454927	5954.716141	7.979776	-0.040561	4.174236
197.635354	5962.744349	7.984781	-0.040600	4.176950
197.848906	5970.743455	7.989786	-0.040645	4.179652
198.030119	5978.715567	7.994790	-0.040684	4.182343
198.288141	5986.763571	7.999795	-0.040737	4.185059
198.419295	5994.827532	8.004800	-0.040767	4.187777
198.467042	6002.817858	8.009805	-0.040781	4.190468
198.831535	6010.944260	8.014810	-0.040854	4.193206
198.999420	6018.914288	8.019814	-0.040891	4.195887
199.000064	6026.896659	8.024819	-0.040896	4.198569
199.274965	6034.920130	8.029824	-0.040953	4.201267
199.362567	6042.878437	8.034829	-0.040974	4.203938
199.512522	6050.930237	8.039834	-0.041008	4.206640
199.473251	6058.879459	8.044838	-0.041005	4.209304
199.589677	6066.966916	8.049843	-0.041032	4.212013
199.783302	6074.974233	8.054848	-0.041074	4.214696
199.753863	6082.992585	8.059853	-0.041073	4.217377
200.170879	6090.989473	8.064858	-0.041156	4.220055
200.293385	6098.982692	8.069862	-0.041184	4.222726
200.185069	6107.032813	8.074867	-0.041170	4.225413
200.464288	6115.054078	8.079872	-0.041227	4.228092
200.748519	6123.061672	8.084877	-0.041285	4.230764
200.883613	6131.107866	8.089882	-0.041315	4.233447
200.879210	6139.113570	8.094886	-0.041320	4.236113
201.376123	6147.105175	8.099891	-0.041418	4.238777
201.565998	6155.128654	8.104896	-0.041458	4.241447
201.413082	6163.091855	8.109901	-0.041435	4.244093
201.877077	6171.161947	8.114906	-0.041527	4.246778
201.824413	6179.165284	8.119910	-0.041522	4.249434
201.960557	6187.214483	8.124915	-0.041553	4.252105
202.157409	6195.269012	8.129920	-0.041595	4.254777
202.478373	6203.246104	8.134925	-0.041660	4.257423
202.616022	6211.291775	8.139930	-0.041691	4.260089
202.528479	6219.286357	8.144934	-0.041680	4.262733
203.000859	6227.292540	8.149939	-0.041773	4.265385
202.949725	6235.326385	8.154944	-0.041768	4.268040
202.966529	6243.354908	8.159949	-0.041777	4.270691
203.241169	6251.415714	8.164954	-0.041833	4.273355
203.384712	6259.487931	8.169958	-0.041865	4.276019
203.588505	6267.400747	8.174963	-0.041908	4.278629
203.765335	6275.449989	8.179968	-0.041947	4.281282
203.870876	6283.395149	8.184973	-0.041972	4.283899
204.006199	6291.499163	8.189978	-0.042002	4.286567
204.133519	6299.434698	8.194982	-0.042031	4.289177
204.125431	6307.527696	8.199987	-0.042035	4.291837
204.392407	6315.555203	8.204992	-0.042090	4.294476
204.496479	6323.482347	8.209997	-0.042114	4.297079
204.696878	6331.541476	8.215002	-0.042157	4.299724
205.027847	6339.609169	8.220006	-0.042224	4.302371
205.025900	6347.590820	8.225011	-0.042229	4.304986
205.157447	6355.628522	8.230016	-0.042258	4.307619
205.410144	6363.614901	8.235021	-0.042311	4.310234
205.591697	6371.680481	8.240026	-0.042350	4.312873
205.766862	6379.677653	8.245030	-0.042388	4.315488
205.832773	6387.684178	8.250035	-0.042405	4.318104
206.099920	6395.730228	8.255040	-0.042460	4.320733
206.160662	6403.649066	8.260045	-0.042477	4.323316
206.410235	6411.727447	8.265050	-0.042529	4.325952
206.513061	6419.729779	8.270054	-0.042553	4.328560
206.615282	6427.755222	8.275059	-0.042577	4.331174
206.758631	6435.823050	8.280064	-0.042609	4.333801
206.931469	6443.833745	8.285069	-0.042647	4.336407
207.135953	6451.781403	8.290074	-0.042690	4.338992
207.257166	6459.826027	8.295078	-0.042718	4.341606
207.777402	6467.804630	8.300083	-0.042820	4.344200
207.740302	6475.859518	8.305088	-0.042818	4.346813
207.618486	6483.896918	8.310093	-0.042801	4.349418
208.002592	6491.962473	8.315098	-0.042878	4.352034
208.215422	6499.988300	8.320102	-0.042923	4.354635
208.288479	6507.992877	8.325107	-0.042941	4.357226
208.313186	6515.941430	8.330112	-0.042951	4.359798
208.527103	6523.911252	8.335117	-0.042996	4.362375
209.015986	6531.936585	8.340122	-0.043093	4.364971
208.940200	6539.973928	8.345126	-0.043084	4.367566
209.080251	6547.977064	8.350131	-0.043115	4.370149
209.346181	6556.056214	8.355136	-0.043170	4.372757
209.311717	6564.069377	8.360141	-0.043169	4.375339
209.384636	6572.083340	8.365146	-0.043188	4.377921
209.624100	6580.067007	8.370150	-0.043237	4.380493
209.798535	6588.051794	8.375155	-0.043275	4.383063
209.931579	6596.103274	8.380160	-0.043305	4.385652
210.051159	6604.117054	8.385165	-0.043333	4.388228
210.225886	6612.175470	8.390170	-0.043371	4.390817
210.346944	6620.186140	8.395174	-0.043398	4.393389
210.340920	6628.217369	8.400179	-0.043402	4.395966
210.716552	6636.226384	8.405184	-0.043478	4.398535
210.795573	6644.211101	8.410189	-0.043498	4.401094
210.899260	6652.184491	8.415194	-0.043522	4.403648
211.114075	6660.227093	8.420198	-0.043567	4.406223
211.294652	6668.231110	8.425203	-0.043606	4.408784
211.163769	6676.306390	8.430208	-0.043587	4.411365
211.287897	6684.263067	8.435213	-0.043616	4.413907
211.552274	6692.344463	8.440218	-0.043670	4.416489
211.584870	6700.292363	8.445222	-0.043681	4.419025
211.597566	6708.379309	8.450227	-0.043689	4.421604
211.980021	6716.362556	8.455232	-0.043765	4.424150
211.935027	6724.367682	8.460237	-0.043762	4.426700
212.172188	6732.425276	8.465242	-0.043812	4.429266
212.246027	6740.445835	8.470246	-0.043831	4.431819
212.480421	6748.470732	8.475251	-0.043880	4.434372
212.601348	6756.518653	8.480256	-0.043907	4.436930
212.767820	6764.450689	8.485261	-0.043944	4.439450
213.042397	6772.514707	8.490266	-0.044000	4.442011
213.164321	6780.449707	8.495270	-0.044028	4.444529
213.187951	6788.489060	8.500275	-0.044038	4.447078
213.382268	6796.534753	8.505280	-0.044079	4.449628
213.754503	6804.556233	8.510285	-0.044154	4.452170
213.592986	6812.604021	8.515290	-0.044129	4.454717
213.695680	6820.629365	8.520294	-0.044153	4.457256
213.797942	6828.598098	8.525299	-0.044178	4.459776
214.099497	6836.663854	8.530304	-0.044239	4.462325
214.131879	6844.612954	8.535309	-0.044250	4.464836
214.375849	6852.678847	8.540314	-0.044301	4.467382
214.313168	6860.684666	8.545318	-0.044295	4.469907
214.324406	6868.709018	8.550323	-0.044302	4.472437
214.609247	6876.707128	8.555328	-0.044360	4.474958
214.752161	6884.685635	8.560333	-0.044392	4.477471
215.040610	6892.715748	8.565338	-0.044451	4.479999
215.199975	6900.754858	8.570343	-0.044486	4.482528
215.349358	6908.749011	8.575347	-0.044519	4.485042
215.357528	6916.811770	8.580352	-0.044526	4.487575
215.385604	6924.793368	8.585357	-0.044536	4.490081
215.777782	6932.835594	8.590362	-0.044615	4.492607
215.753656	6940.881513	8.595367	-0.044615	4.495130
215.920382	6948.823567	8.600371	-0.044652	4.497620
216.149614	6956.871192	8.605376	-0.044700	4.500142
216.210143	6964.832194	8.610381	-0.044716	4.502635
216.415317	6972.882186	8.615386	-0.044760	4.505155
216.600308	6980.919974	8.620391	-0.044799	4.507669
216.725194	6988.936861	8.625395	-0.044828	4.510176
216.881460	6997.007986	8.630400	-0.044862	4.512698
216.922912	7005.030607	8.635405	-0.044875	4.515203
217.191673	7013.011900	8.640410	-0.044930	4.517694
217.362458	7020.954403	8.645415	-0.044967	4.520172
217.376344	7028.970627	8.650419	-0.044975	4.522671
217.738432	7036.979758	8.655424	-0.045048	4.525167
217.925019	7044.995699	8.660429	-0.045088	4.527663
218.135362	7053.058129	8.665434	-0.045132	4.530172
217.896492	7061.087946	8.670439	-0.045093	4.532669
218.204245	7069.059303	8.675443	-0.045156	4.535148
218.500030	7077.089504	8.680448	-0.045216	4.537643
218.456527	7085.095130	8.685453	-0.045213	4.540129
218.724898	7093.135503	8.690458	-0.045269	4.542625
218.640260	7101.089787	8.695463	-0.045258	4.545092
218.715138	7109.112972	8.700467	-0.045277	4.547579
218.890565	7117.166262	8.705472	-0.045315	4.550075
218.977147	7125.206349	8.710477	-0.045337	4.552564
219.248503	7133.239883	8.715482	-0.045392	4.555051
219.447738	7141.249992	8.720487	-0.045435	4.557529
219.675064	7149.205830	8.725491	-0.045482	4.559989
219.848492	7157.276461	8.730496	-0.045520	4.562483
219.650250	7165.247943	8.735501	-0.045488	4.564944
219.774632	7173.341784	8.740506	-0.045517	4.567442
219.974270	7181.304176	8.745511	-0.045559	4.569899
220.285768	7189.328277	8.750515	-0.045622	4.572373
220.377098	7197.366712	8.755520	-0.045645	4.574850
220.362534	7205.360193	8.760525	-0.045647	4.577312
220.491640	7213.376832	8.765530	-0.045676	4.579779
220.746661	7221.391414	8.770535	-0.045729	4.582245
220.885978	7229.365012	8.775539	-0.045760	4.584697
221.078438	7237.454600	8.780544	-0.045801	4.587183
221.172322	7245.459396	8.785549	-0.045824	4.589641
221.368133	7253.512073	8.790554	-0.045866	4.592113
221.421224	7261.517516	8.795559	-0.045881	4.594569
221.511766	7269.563875	8.800563	-0.045903	4.597037
221.653761	7277.520781	8.805568	-0.045935	4.599475
221.776946	7285.469762	8.810573	-0.045963	4.601910
222.077001	7293.552379	8.815578	-0.046024	4.604385
222.201407	7301.579395	8.820583	-0.046053	4.606841
222.325337	7309.517824	8.825587	-0.046081	4.609268
222.460248	7317.619878	8.830592	-0.046111	4.611745
222.370876	7325.624172	8.835597	-0.046100	4.614190
222.679116	7333.651081	8.840602	-0.046163	4.616641
222.913173	7341.585152	8.845607	-0.046211	4.619062
222.959014	7349.648334	8.850611	-0.046225	4.621521
223.069909	7357.635964	8.855616	-0.046251	4.623956
223.164723	7365.689344	8.860621	-0.046274	4.626409
223.395307	7373.717430	8.865626	-0.046322	4.628854
223.394118	7381.692134	8.870631	-0.046327	4.631281
223.554656	7389.785200	8.875635	-0.046362	4.633743
223.872156	7397.816112	8.880640	-0.046427	4.636184
223.711931	7405.711825	8.885645	-0.046402	4.638583
223.840371	7413.754022	8.890650	-0.046431	4.641026
224.065135	7421.760594	8.895655	-0.046478	4.643456
224.227942	7429.774400	8.900659	-0.046514	4.645887
224.322465	7437.821141	8.905664	-0.046537	4.648327
224.564290	7445.826181	8.910669	-0.046587	4.650753
224.821086	7453.865444	8.915674	-0.046640	4.653187
224.849940	7461.886662	8.920679	-0.046651	4.655616
225.092189	7469.882854	8.925683	-0.046701	4.658035
225.369676	7477.893754	8.930688	-0.046758	4.660457
225.350836	7485.866526	8.935693	-0.046760	4.662867
225.248968	7493.908224	8.940698	-0.046746	4.665297
225.484612	7501.950280	8.945703	-0.046795	4.667725
225.635764	7509.940385	8.950707	-0.046829	4.670136
225.841111	7518.045705	8.955712	-0.046872	4.672580
225.919756	7526.078117	8.960717	-0.046892	4.675002
226.152923	7534.079204	8.965722	-0.046941	4.677412
226.310174	7541.995995	8.970727	-0.046975	4.679796
226.402607	7550.033786	8.975731	-0.046998	4.682215
226.650707	7558.004998	8.980736	-0.047049	4.684613
226.540958	7566.030318	8.985741	-0.047034	4.687026
226.747050	7574.020009	8.990746	-0.047078	4.689427
226.905290	7582.125875	8.995751	-0.047112	4.691862
227.155574	7590.079524	9.000755	-0.047164	4.694249
227.234437	7598.139262	9.005760	-0.047184	4.696668
227.324005	7606.089767	9.010765	-0.047206	4.699052
227.472454	7614.193725	9.015770	-0.047239	4.701481
227.676476	7622.101159	9.020775	-0.047282	4.703849
227.703998	7630.143842	9.025779	-0.047293	4.706258
227.899899	7638.223204	9.030784	-0.047334	4.708675
227.798199	7646.216864	9.035789	-0.047321	4.711067
228.022885	7654.260951	9.040794	-0.047368	4.713471
228.158757	7662.260465	9.045799	-0.047398	4.715862
228.470189	7670.243570	9.050803	-0.047462	4.718245
228.667653	7678.303115	9.055808	-0.047504	4.720651
228.706201	7686.287004	9.060813	-0.047516	4.723033
228.944179	7694.306006	9.065818	-0.047566	4.725424
228.929545	7702.326916	9.070823	-0.047568	4.727815
229.073908	7710.348096	9.075827	-0.047600	4.730204
229.271813	7718.386478	9.080832	-0.047642	4.732597
229.155352	7726.420780	9.085837	-0.047626	4.734988
229.369956	7734.396179	9.090842	-0.047671	4.737360
229.593518	7742.394659	9.095847	-0.047718	4.739737
229.608666	7750.417216	9.100851	-0.047726	4.742121
229.835201	7758.427071	9.105856	-0.047774	4.744500
229.923699	7766.443801	9.110861	-0.047795	4.746879
230.071617	7774.467336	9.115866	-0.047828	4.749260
230.163844	7782.511203	9.120871	-0.047851	4.751645
230.304666	7790.571282	9.125875	-0.047882	4.754033
230.661624	7798.578882	9.130880	-0.047954	4.756405
230.700568	7806.486795	9.135885	-0.047966	4.758746
230.804705	7814.578754	9.140890	-0.047991	4.761141
231.063966	7822.482431	9.145895	-0.048044	4.763478
231.119244	7830.521776	9.150899	-0.048060	4.765855
231.180998	7838.582151	9.155904	-0.048077	4.768236
231.192751	7846.608963	9.160909	-0.048084	4.770607
231.568467	7854.646487	9.165914	-0.048160	4.772979
231.648410	7862.674848	9.170919	-0.048180	4.775347
231.625345	7870.657187	9.175923	-0.048181	4.777702
231.610083	7878.632972	9.180928	-0.048183	4.780053
231.771461	7886.680764	9.185933	-0.048218	4.782423
232.087492	7894.622318	9.190938	-0.048282	4.784761
232.066305	7902.726619	9.195943	-0.048284	4.787146
232.262921	7910.676664	9.200947	-0.048326	4.789484
232.516229	7918.791841	9.205952	-0.048378	4.791870
232.491115	7926.767975	9.210957	-0.048379	4.794214
232.671782	7934.821170	9.215962	-0.048418	4.796579
232.805038	7942.729880	9.220967	-0.048448	4.798900
232.998337	7950.774258	9.225971	-0.048489	4.801260
233.334160	7958.817383	9.230976	-0.048557	4.803618
233.407582	7966.807313	9.235981	-0.048576	4.805960
233.346538	7974.854503	9.240986	-0.048569	4.808318
233.583117	7982.823947	9.245991	-0.048619	4.810652
233.624141	7990.317428	9.250995	-0.048631	4.812845
233.724457	7995.024872	9.256000	-0.048653	4.814222

233.646410	7997.608087	9.261005	-0.048640	4.814978
233.895828	7998.959992	9.266010	-0.048688	4.815373
234.121101	7999.365989	9.271015	-0.048730	4.815490
233.991336	8000.445094	9.276019	-0.048706	4.815807
234.277552	8000.467867	9.281024	-0.048760	4.815812
234.265442	8000.469809	9.286029	-0.048758	4.815813
234.072187	8000.466689	9.291034	-0.048722	4.815813
234.123518	8000.441905	9.296039	-0.048731	4.815805
234.304197	8000.437356	9.301043	-0.048765	4.815803
234.280295	8000.470061	9.306048	-0.048760	4.815813
234.237624	8000.445892	9.311053	-0.048753	4.815806
234.406350	8000.473171	9.316058	-0.048784	4.815813
234.533364	8000.449610	9.321063	-0.048808	4.815805
234.490015	8000.469192	9.326067	-0.048800	4.815811
234.472355	8000.447563	9.331072	-0.048796	4.815805
234.468694	8000.422957	9.336077	-0.048796	4.815798
234.491216	8000.462816	9.341082	-0.048800	4.815809
234.560421	8000.458601	9.346087	-0.048813	4.815808
234.672929	8000.447614	9.351091	-0.048834	4.815804
234.824635	8000.479955	9.356096	-0.048862	4.815813
234.713470	8000.436534	9.361101	-0.048841	4.815801
234.582493	8000.454700	9.366106	-0.048817	4.815807
234.884045	8000.444634	9.371111	-0.048873	4.815802
234.880980	8000.429644	9.376115	-0.048873	4.815798
234.737238	8000.449738	9.381120	-0.048846	4.815804
234.919609	8000.426005	9.386125	-0.048880	4.815797
234.923299	8000.471965	9.391130	-0.048881	4.815810
234.978720	8000.453651	9.396135	-0.048891	4.815804
234.849877	8000.483592	9.401139	-0.048867	4.815814
234.940653	8000.491467	9.406144	-0.048884	4.815816
234.748267	8000.464878	9.411149	-0.048848	4.815809
235.029520	8000.453416	9.416154	-0.048901	4.815804
235.051585	8000.429226	9.421159	-0.048905	4.815797
234.998551	8000.446517	9.426163	-0.048895	4.815802
235.063856	8000.463587	9.431168	-0.048907	4.815807
235.212392	8000.458519	9.436173	-0.048935	4.815805
235.119689	8000.484775	9.441178	-0.048918	4.815813
235.148082	8000.463890	9.446183	-0.048923	4.815807
235.256679	8000.462446	9.451187	-0.048943	4.815806
235.383712	8000.485851	9.456192	-0.048967	4.815812
235.113300	8000.438786	9.461197	-0.048917	4.815799
235.246680	8000.482574	9.466202	-0.048941	4.815812
235.183047	8000.459133	9.471207	-0.048930	4.815805
235.257637	8000.465679	9.476211	-0.048944	4.815807
235.104723	8000.479220	9.481216	-0.048915	4.815811
235.146278	8000.455345	9.486221	-0.048923	4.815804
235.254931	8000.460307	9.491226	-0.048943	4.815805
235.225740	8000.461973	9.496231	-0.048938	4.815806
235.184937	8000.473057	9.501235	-0.048930	4.815809
235.275874	8000.487339	9.506240	-0.048947	4.815813
235.335602	8000.436006	9.511245	-0.048958	4.815798
235.378221	8000.460180	9.516250	-0.048966	4.815804
235.425367	8000.440665	9.521255	-0.048975	4.815798
235.363457	8000.426858	9.526259	-0.048964	4.815795
235.380870	8000.474108	9.531264	-0.048967	4.815808
235.562160	8000.437548	9.536269	-0.049001	4.815797
235.500534	8000.469644	9.541274	-0.048989	4.815807
235.402385	8000.457386	9.546279	-0.048971	4.815803
235.179330	8000.450581	9.551283	-0.048929	4.815803
235.411749	8000.469285	9.556288	-0.048973	4.815807
235.391539	8000.434805	9.561293	-0.048969	4.815797
235.428964	8000.475974	9.566298	-0.048976	4.815809
235.448933	8000.444278	9.571303	-0.048980	4.815799
235.381536	8000.456000	9.576307	-0.048967	4.815803
235.538552	8000.460676	9.581312	-0.048997	4.815804
235.587854	8000.424117	9.586317	-0.049006	4.815793
235.636019	8000.443045	9.591322	-0.049015	4.815798
235.604942	8000.444680	9.596327	-0.049009	4.815799
235.334014	8000.455246	9.601331	-0.048959	4.815803
235.465216	8000.470179	9.606336	-0.048983	4.815807
235.444730	8000.432492	9.611341	-0.048979	4.815796
235.461537	8000.450912	9.616346	-0.048982	4.815801
235.551732	8000.444902	9.621351	-0.048999	4.815799
235.473030	8000.453239	9.626355	-0.048985	4.815802
235.642228	8000.473056	9.631360	-0.049016	4.815807
235.543046	8000.434096	9.636365	-0.048998	4.815796
235.915041	8000.477473	9.641370	-0.049067	4.815807
235.717663	8000.440128	9.646375	-0.049030	4.815797
235.633189	8000.450506	9.651379	-0.049015	4.815800
235.849141	8000.450799	9.656384	-0.049055	4.815799
235.862460	8000.455287	9.661389	-0.049057	4.815801
235.617022	8000.466265	9.666394	-0.049012	4.815805
235.730844	8000.476647	9.671399	-0.049033	4.815808
235.603396	8000.467118	9.676403	-0.049009	4.815805
235.841596	8000.458164	9.681408	-0.049054	4.815802
235.691099	8000.432250	9.686413	-0.049026	4.815795
235.812281	8000.420337	9.691418	-0.049048	4.815791
235.879656	8000.437440	9.696423	-0.049061	4.815795
235.769865	8000.458083	9.701427	-0.049040	4.815802
235.823131	8000.486700	9.706432	-0.049050	4.815810
235.931638	8000.443626	9.711437	-0.049071	4.815797
235.959055	8000.477162	9.716442	-0.049076	4.815807
236.057214	8000.433922	9.721447	-0.049094	4.815793
235.955537	8000.434415	9.726451	-0.049075	4.815794
235.829609	8000.477213	9.731456	-0.049052	4.815807
235.623791	8000.463214	9.736461	-0.049014	4.815804
235.724039	8000.496860	9.741466	-0.049032	4.815813
235.941929	8000.467297	9.746471	-0.049073	4.815804
235.809931	8000.463030	9.751475	-0.049048	4.815803
235.684163	8000.474876	9.756480	-0.049025	4.815807
235.736205	8000.449035	9.761485	-0.049035	4.815799
235.611954	8000.476916	9.766490	-0.049012	4.815808
235.710480	8000.471040	9.771495	-0.049030	4.815806
235.858424	8000.425403	9.776499	-0.049057	4.815792
235.897282	8000.468730	9.781504	-0.049065	4.815804
235.978705	8000.439095	9.786509	-0.049080	4.815795
235.924867	8000.454238	9.791514	-0.049070	4.815800
235.949761	8000.430094	9.796519	-0.049075	4.815793
235.836770	8000.414393	9.801523	-0.049054	4.815789
236.121249	8000.439277	9.806528	-0.049107	4.815795
235.868038	8000.440523	9.811533	-0.049060	4.815796
235.713095	8000.479649	9.816538	-0.049031	4.815808
235.592803	8000.454224	9.821543	-0.049008	4.815802
235.908942	8000.423047	9.826547	-0.049067	4.815791
235.768718	8000.470950	9.831552	-0.049041	4.815806
235.652846	8000.425316	9.836557	-0.049020	4.815793
235.825431	8000.465469	9.841562	-0.049052	4.815804
235.960105	8000.446302	9.846567	-0.049077	4.815798
235.689360	8000.434455	9.851571	-0.049027	4.815795
235.777449	8000.468972	9.856576	-0.049043	4.815805
236.029994	8000.455980	9.861581	-0.049090	4.815800
236.167730	8000.452873	9.866586	-0.049116	4.815798
236.108465	8000.454053	9.871591	-0.049105	4.815799
235.874785	8000.436401	9.876595	-0.049061	4.815795
236.333106	8000.441681	9.881600	-0.049147	4.815794
236.135335	8000.426744	9.886605	-0.049110	4.815791
235.996192	8000.465058	9.891610	-0.049084	4.815803
236.113127	8000.461615	9.896615	-0.049106	4.815801
235.931030	8000.482156	9.901619	-0.049072	4.815808
235.973727	8000.506332	9.906624	-0.049080	4.815815
236.097970	8000.428289	9.911629	-0.049103	4.815792
236.040573	8000.457251	9.916634	-0.049092	4.815800
236.003778	8000.460929	9.921639	-0.049086	4.815802
236.025667	8000.471960	9.926643	-0.049090	4.815805
235.979141	8000.463738	9.931648	-0.049081	4.815803
235.856566	8000.454287	9.936653	-0.049058	4.815800
236.092360	8000.451699	9.941658	-0.049102	4.815798
236.216223	8000.460110	9.946663	-0.049125	4.815800
236.123194	8000.459675	9.951667	-0.049108	4.815801
236.152706	8000.463358	9.956672	-0.049114	4.815802
236.205006	8000.453533	9.961677	-0.049123	4.815798
236.232989	8000.490280	9.966682	-0.049129	4.815809
236.073468	8000.459951	9.971687	-0.049099	4.815801
236.017209	8000.455842	9.976691	-0.049088	4.815800
236.251360	8000.488451	9.981696	-0.049132	4.815808
236.161856	8000.476333	9.986701	-0.049115	4.815805
236.191133	8000.465068	9.991706	-0.049121	4.815802
236.290176	8000.476279	9.996711	-0.049139	4.815805
236.072712	8000.443945	10.001715	-0.049099	4.815796
236.116768	8000.491627	10.006720	-0.049107	4.815810
236.199224	8000.458806	10.011725	-0.049123	4.815800
236.219923	8000.495436	10.016730	-0.049126	4.815811
236.149221	8000.463340	10.021735	-0.049113	4.815802
236.122156	8000.463973	10.026739	-0.049108	4.815802
236.336855	8000.485594	10.031744	-0.049148	4.815807
236.088755	8000.463439	10.036749	-0.049102	4.815802
236.149805	8000.498586	10.041754	-0.049114	4.815812
236.442394	8000.489445	10.046759	-0.049168	4.815808
236.380827	8000.452160	10.051763	-0.049157	4.815797
236.268454	8000.491975	10.056768	-0.049136	4.815809
236.158667	8000.459247	10.061773	-0.049115	4.815800
236.235517	8000.456223	10.066778	-0.049130	4.815799
236.211479	8000.452635	10.071783	-0.049125	4.815798
236.152563	8000.466629	10.076787	-0.049114	4.815803
236.388597	8000.500337	10.081792	-0.049158	4.815811
236.309362	8000.458497	10.086797	-0.049144	4.815799
236.231531	8000.487129	10.091802	-0.049129	4.815808
236.286410	8000.451727	10.096807	-0.049139	4.815798
236.138573	8000.444002	10.101811	-0.049112	4.815796
236.389120	8000.477945	10.106816	-0.049159	4.815805
236.447995	8000.468226	10.111821	-0.049170	4.815802
236.396784	8000.443917	10.116826	-0.049160	4.815795
236.375696	8000.436107	10.121831	-0.049156	4.815793
236.319316	8000.436266	10.126835	-0.049146	4.815793
236.462508	8000.475944	10.131840	-0.049172	4.815804
236.352597	8000.470967	10.136845	-0.049152	4.815803
236.318919	8000.459752	10.141850	-0.049146	4.815800
236.478200	8000.483679	10.146855	-0.049175	4.815806
236.359944	8000.460421	10.151859	-0.049153	4.815800
236.396567	8000.461016	10.156864	-0.049160	4.815800
236.247757	8000.416983	10.161869	-0.049133	4.815788
236.357122	8000.458249	10.166874	-0.049153	4.815799
236.466553	8000.472831	10.171879	-0.049173	4.815803
236.404672	8000.450485	10.176883	-0.049162	4.815797
236.412288	8000.482634	10.181888	-0.049163	4.815806
236.553014	8000.441149	10.186893	-0.049190	4.815793
236.512731	8000.475725	10.191898	-0.049182	4.815803
236.561037	8000.469037	10.196903	-0.049191	4.815801
236.479284	8000.458111	10.201907	-0.049176	4.815798
236.485183	8000.479558	10.206912	-0.049177	4.815805
236.483569	8000.438973	10.211917	-0.049177	4.815793
236.617952	8000.458228	10.216922	-0.049202	4.815798
236.390746	8000.469500	10.221927	-0.049160	4.815802
236.471324	8000.456930	10.226931	-0.049175	4.815798
236.446201	8000.486414	10.231936	-0.049170	4.815807
236.524986	8000.447130	10.236941	-0.049185	4.815795
236.471249	8000.485758	10.241946	-0.049175	4.815807
236.621042	8000.443352	10.246951	-0.049203	4.815793
236.591272	8000.475964	10.251955	-0.049197	4.815803
236.278130	8000.496520	10.256960	-0.049139	4.815811
236.360683	8000.465835	10.261965	-0.049154	4.815801
236.579240	8000.448025	10.266970	-0.049195	4.815795
236.641105	8000.452231	10.271975	-0.049207	4.815796
236.527115	8000.415165	10.276979	-0.049185	4.815786
236.629680	8000.445648	10.281984	-0.049205	4.815794
236.604179	8000.448440	10.286989	-0.049200	4.815795
236.522022	8000.478070	10.291994	-0.049185	4.815804
236.691530	8000.476545	10.296999	-0.049216	4.815803
236.713034	8000.463019	10.302003	-0.049220	4.815799
236.756192	8000.497878	10.307008	-0.049228	4.815809
236.627950	8000.482997	10.312013	-0.049204	4.815805
236.619571	8000.504213	10.317018	-0.049203	4.815811
236.498538	8000.488382	10.322023	-0.049180	4.815807
236.476914	8000.446406	10.327027	-0.049176	4.815795
236.662998	8000.492115	10.332032	-0.049211	4.815808
236.681373	8000.481741	10.337037	-0.049215	4.815804
236.602595	8000.474065	10.342042	-0.049200	4.815803
236.628515	8000.456342	10.347047	-0.049205	4.815797
236.519843	8000.456721	10.352051	-0.049185	4.815798
236.638848	8000.490672	10.357056	-0.049207	4.815807
236.706252	8000.424518	10.362061	-0.049219	4.815788
236.923019	8000.408814	10.367066	-0.049260	4.815782
236.665538	8000.439876	10.372071	-0.049212	4.815792
236.543367	8000.412285	10.377075	-0.049189	4.815785
236.794412	8000.483597	10.382080	-0.049236	4.815804
236.691652	8000.433903	10.387085	-0.049217	4.815790
236.440533	8000.383946	10.392090	-0.049170	4.815777
236.530654	8000.451586	10.397095	-0.049187	4.815796
236.605274	8000.412234	10.402099	-0.049201	4.815784
236.561660	8000.447824	10.407104	-0.049193	4.815795
236.512563	8000.455572	10.412109	-0.049184	4.815798
236.675193	8000.488093	10.417114	-0.049214	4.815806
236.553715	8000.487199	10.422119	-0.049191	4.815807
236.603597	8000.419694	10.427123	-0.049201	4.815787
236.769999	8000.489636	10.432128	-0.049232	4.815806
236.696060	8000.439341	10.437133	-0.049218	4.815792
236.682442	8000.475416	10.442138	-0.049215	4.815803
236.631931	8000.490614	10.447143	-0.049206	4.815807
236.420204	8000.450900	10.452147	-0.049167	4.815797
236.664452	8000.472999	10.457152	-0.049212	4.815802
236.620894	8000.432803	10.462157	-0.049204	4.815790
236.527345	8000.453709	10.467162	-0.049187	4.815797
236.645298	8000.488710	10.472167	-0.049209	4.815807
236.612241	8000.472167	10.477171	-0.049203	4.815802
236.705300	8000.493956	10.482176	-0.049220	4.815808
236.390751	8000.452579	10.487181	-0.049161	4.815797
236.556060	8000.483009	10.492186	-0.049192	4.815805
236.515945	8000.462082	10.497191	-0.049185	4.815799
236.341710	8000.444323	10.502195	-0.049152	4.815795
236.625534	8000.469197	10.507200	-0.049205	4.815801
236.445954	8000.421464	10.512205	-0.049172	4.815788
236.588694	8000.455798	10.517210	-0.049199	4.815797
236.712882	8000.461012	10.522215	-0.049222	4.815798
236.632644	8000.383931	10.527219	-0.049207	4.815776
236.783242	8000.455752	10.532224	-0.049235	4.815796
236.906274	8000.439599	10.537229	-0.049258	4.815791
236.861724	8000.473039	10.542234	-0.049250	4.815801
236.960936	8000.495996	10.547239	-0.049268	4.815807
236.749471	8000.493645	10.552243	-0.049229	4.815808
236.688646	8000.499068	10.557248	-0.049217	4.815809
236.623423	8000.465994	10.562253	-0.049205	4.815800
236.718633	8000.464334	10.567258	-0.049223	4.815799
236.773018	8000.495105	10.572263	-0.049233	4.815808
236.593408	8000.470854	10.577267	-0.049200	4.815802
236.662553	8000.491189	10.582272	-0.049213	4.815807
236.839786	8000.446025	10.587277	-0.049246	4.815793
236.691141	8000.482051	10.592282	-0.049218	4.815804
236.772621	8000.488709	10.597287	-0.049233	4.815806
236.598213	8000.452800	10.602291	-0.049201	4.815796
236.672799	8000.452942	10.607296	-0.049215	4.815796
236.817511	8000.455286	10.612301	-0.049242	4.815796
236.897112	8000.474723	10.617306	-0.049257	4.815801
237.015514	8000.463833	10.622311	-0.049279	4.815798
236.612168	8000.447704	10.627315	-0.049204	4.815795
236.710676	8000.462109	10.632320	-0.049222	4.815798
236.777605	8000.449319	10.637325	-0.049235	4.815794
236.665097	8000.452839	10.642330	-0.049214	4.815796
236.506917	8000.473766	10.647335	-0.049184	4.815803
236.517006	8000.442977	10.652339	-0.049186	4.815794
236.735144	8000.492408	10.657344	-0.049227	4.815807
236.647451	8000.471779	10.662349	-0.049210	4.815802
236.451379	8000.480352	10.667354	-0.049174	4.815805
236.816762	8000.489468	10.672359	-0.049242	4.815806
236.721584	8000.451638	10.677363	-0.049224	4.815795
236.695519	8000.458692	10.682368	-0.049220	4.815798
236.738474	8000.431636	10.687373	-0.049228	4.815789
236.919344	8000.477263	10.692378	-0.049261	4.815802
236.719511	8000.475100	10.697383	-0.049224	4.815802
236.785725	8000.464432	10.702387	-0.049236	4.815799
236.834418	8000.504718	10.707392	-0.049246	4.815810
236.808026	8000.485080	10.712397	-0.049241	4.815805
236.686971	8000.490597	10.717402	-0.049218	4.815807
236.808733	8000.485098	10.722407	-0.049241	4.815805
236.685601	8000.485244	10.727411	-0.049218	4.815805
236.628630	8000.519550	10.732416	-0.049207	4.815816
236.783708	8000.486837	10.737421	-0.049236	4.815805
236.663498	8000.497704	10.742426	-0.049214	4.815809
236.735966	8000.489272	10.747431	-0.049228	4.815806
236.747395	8000.457438	10.752435	-0.049230	4.815797
236.925260	8000.485936	10.757440	-0.049263	4.815804
236.703264	8000.483415	10.762445	-0.049222	4.815805
236.628188	8000.503552	10.767450	-0.049208	4.815811
236.867594	8000.494619	10.772455	-0.049252	4.815807
236.821479	8000.451179	10.777459	-0.049244	4.815795
236.744839	8000.491572	10.782464	-0.049229	4.815807
236.808527	8000.484065	10.787469	-0.049241	4.815804
236.984326	8000.481575	10.792474	-0.049274	4.815803
236.810641	8000.478768	10.797479	-0.049242	4.815803
236.894800	8000.438503	10.802483	-0.049257	4.815791
237.079511	8000.509810	10.807488	-0.049292	4.815811
236.878038	8000.474531	10.812493	-0.049254	4.815801
236.735366	8000.480765	10.817498	-0.049228	4.815804
236.880882	8000.500201	10.822503	-0.049255	4.815809
236.797434	8000.472168	10.827507	-0.049240	4.815801
236.806068	8000.490457	10.832512	-0.049241	4.815806
236.724539	8000.430433	10.837517	-0.049226	4.815789
236.839592	8000.478196	10.842522	-0.049247	4.815803
236.975029	8000.465446	10.847527	-0.049273	4.815798
236.829790	8000.419335	10.852531	-0.049246	4.815785
237.106126	8000.495327	10.857536	-0.049297	4.815806
237.203103	8000.468078	10.862541	-0.049315	4.815798
236.930936	8000.480756	10.867546	-0.049265	4.815803
236.991530	8000.489212	10.872551	-0.049276	4.815805
237.038238	8000.475026	10.877555	-0.049285	4.815801
237.041827	8000.504975	10.882560	-0.049285	4.815809
236.797583	8000.451925	10.887565	-0.049240	4.815795
236.858386	8000.482800	10.892570	-0.049251	4.815804
236.930700	8000.480770	10.897575	-0.049265	4.815803
236.850654	8000.461332	10.902579	-0.049250	4.815798
237.024440	8000.480158	10.907584	-0.049282	4.815802
236.997708	8000.460515	10.912589	-0.049277	4.815797
236.860870	8000.461506	10.917594	-0.049252	4.815798
236.997139	8000.503209	10.922599	-0.049277	4.815809
236.871019	8000.458474	10.927603	-0.049254	4.815797
236.943076	8000.492733	10.932608	-0.049267	4.815806
237.006779	8000.473485	10.937613	-0.049279	4.815800
236.992678	8000.482867	10.942618	-0.049277	4.815803
237.048469	8000.493380	10.947623	-0.049287	4.815806
236.909824	8000.479398	10.952627	-0.049261	4.815803
237.090309	8000.507939	10.957632	-0.049295	4.815810
236.986761	8000.481716	10.962637	-0.049276	4.815803
236.818865	8000.464058	10.967642	-0.049244	4.815798
236.837072	8000.486772	10.972647	-0.049248	4.815805
236.872703	8000.441452	10.977651	-0.049255	4.815792
237.024132	8000.500479	10.982656	-0.049283	4.815808
236.982528	8000.500876	10.987661	-0.049275	4.815808
237.090507	8000.458861	10.992666	-0.049295	4.815796
237.237449	8000.497535	10.997671	-0.049323	4.815806
236.866831	8000.479799	11.002675	-0.049254	4.815803
237.161059	8000.481360	11.007680	-0.049308	4.815802
237.159674	8000.465329	11.012685	-0.049308	4.815797
237.042405	8000.429277	11.017690	-0.049286	4.815787
237.293274	8000.431204	11.022695	-0.049333	4.815787
237.183535	8000.444376	11.027699	-0.049313	4.815791
237.281819	8000.515352	11.032704	-0.049331	4.815811
236.957827	8000.499439	11.037709	-0.049271	4.815808
237.010438	8000.498158	11.042714	-0.049281	4.815808
237.102112	8000.503914	11.047719	-0.049298	4.815809
236.754943	8000.463075	11.052723	-0.049233	4.815798
236.888065	8000.490850	11.057728	-0.049258	4.815806
236.870602	8000.472424	11.062733	-0.049255	4.815801
236.887432	8000.484441	11.067738	-0.049258	4.815804
236.876609	8000.500280	11.072743	-0.049256	4.815809
236.952044	8000.474818	11.077747	-0.049270	4.815801
237.000408	8000.504424	11.082752	-0.049279	4.815809
236.980891	8000.451807	11.087757	-0.049275	4.815794
237.002118	8000.457490	11.092762	-0.049279	4.815796
237.081131	8000.480120	11.097767	-0.049294	4.815802
237.039830	8000.446365	11.102771	-0.049287	4.815792
237.061895	8000.489422	11.107776	-0.049291	4.815805
237.073568	8000.492816	11.112781	-0.049293	4.815806
237.083777	8000.495119	11.117786	-0.049295	4.815806
237.091494	8000.505921	11.122791	-0.049296	4.815809
237.176132	8000.463529	11.127795	-0.049312	4.815797
236.947138	8000.514266	11.132800	-0.049269	4.815813
237.029003	8000.463289	11.137805	-0.049285	4.815797
237.107189	8000.475232	11.142810	-0.049299	4.815800
237.270642	8000.467205	11.147815	-0.049330	4.815797
237.103828	8000.447430	11.152819	-0.049299	4.815792
237.088073	8000.517629	11.157824	-0.049296	4.815813
236.968076	8000.482600	11.162829	-0.049274	4.815803
237.119812	8000.491462	11.167834	-0.049302	4.815805
237.095183	8000.507078	11.172839	-0.049297	4.815810
237.004968	8000.488543	11.177843	-0.049281	4.815805
237.144822	8000.501483	11.182848	-0.049307	4.815808
237.155248	8000.479238	11.187853	-0.049309	4.815801
237.198077	8000.510890	11.192858	-0.049317	4.815810
237.275013	8000.520677	11.197863	-0.049331	4.815813
237.077848	8000.482265	11.202867	-0.049294	4.815803
237.083600	8000.515451	11.207872	-0.049295	4.815812
237.079902	8000.381965	11.212877	-0.049295	4.815773
237.324719	8000.480931	11.217882	-0.049340	4.815801
237.206190	8000.498230	11.222887	-0.049318	4.815807
237.122071	8000.474455	11.227891	-0.049303	4.815800
237.095261	8000.499643	11.232896	-0.049298	4.815808
237.070834	8000.472565	11.237901	-0.049293	4.815800
236.995245	8000.496963	11.242906	-0.049279	4.815807
237.141464	8000.472646	11.247911	-0.049306	4.815799
237.346630	8000.478104	11.252915	-0.049345	4.815800
237.126528	8000.503366	11.257920	-0.049304	4.815808
237.267037	8000.486429	11.262925	-0.049330	4.815803
237.037994	8000.498737	11.267930	-0.049287	4.815808
237.139462	8000.513191	11.272935	-0.049306	4.815811
237.172949	8000.466769	11.277939	-0.049313	4.815798
237.147703	8000.524005	11.282944	-0.049308	4.815814
237.088224	8000.481415	11.287949	-0.049297	4.815802
236.931141	8000.518372	11.292954	-0.049268	4.815814
237.140779	8000.511093	11.297959	-0.049307	4.815811
237.210919	8000.479140	11.302963	-0.049320	4.815801
237.188641	8000.511873	11.307968	-0.049316	4.815811
237.145311	8000.481287	11.312973	-0.049308	4.815802
237.127549	8000.488474	11.317978	-0.049304	4.815804
237.236607	8000.497714	11.322983	-0.049325	4.815806
237.040209	8000.449707	11.327987	-0.049288	4.815793
237.226206	8000.482607	11.332992	-0.049323	4.815802
237.048083	8000.475458	11.337997	-0.049290	4.815801
237.063168	8000.439413	11.343002	-0.049292	4.815790
237.269805	8000.481187	11.348007	-0.049331	4.815801
237.380715	8000.455231	11.353011	-0.049352	4.815793
237.178139	8000.495721	11.358016	-0.049314	4.815806
237.269015	8000.474778	11.363021	-0.049331	4.815799
237.318999	8000.460646	11.368026	-0.049340	4.815795
237.308247	8000.478621	11.373031	-0.049338	4.815800
237.230876	8000.480575	11.378035	-0.049324	4.815801
237.173924	8000.494600	11.383040	-0.049313	4.815806
237.107377	8000.488189	11.388045	-0.049301	4.815804
236.952624	8000.487823	11.393050	-0.049272	4.815805
237.066124	8000.507809	11.398055	-0.049293	4.815810
237.165159	8000.476324	11.403059	-0.049312	4.815800
237.044905	8000.492528	11.408064	-0.049290	4.815806
237.081891	8000.479252	11.413069	-0.049296	4.815802
237.147195	8000.458963	11.418074	-0.049309	4.815795
237.243615	8000.486145	11.423079	-0.049327	4.815803
237.197344	8000.472590	11.428083	-0.049318	4.815799
237.403681	8000.510090	11.433088	-0.049357	4.815809
237.280631	8000.501697	11.438093	-0.049334	4.815807
237.179017	8000.513932	11.443098	-0.049315	4.815811
237.138824	8000.522892	11.448103	-0.049307	4.815814
237.172838	8000.505299	11.453107	-0.049314	4.815809
237.220685	8000.517818	11.458112	-0.049323	4.815812
237.232384	8000.498796	11.463117	-0.049325	4.815807
237.354304	8000.493300	11.468122	-0.049348	4.815804
237.166596	8000.477456	11.473127	-0.049313	4.815801
237.090767	8000.480502	11.478131	-0.049299	4.815802
237.222350	8000.528534	11.483136	-0.049323	4.815815
237.190798	8000.493868	11.488141	-0.049317	4.815805
237.046490	8000.458446	11.493146	-0.049290	4.815796
237.250156	8000.510846	11.498151	-0.049328	4.815810
237.214636	8000.471847	11.503155	-0.049322	4.815799
237.038665	8000.515970	11.508160	-0.049289	4.815813
237.180117	8000.506520	11.513165	-0.049315	4.815809
237.311902	8000.504385	11.518170	-0.049340	4.815808
237.408201	8000.491002	11.523175	-0.049358	4.815803
237.174450	8000.456267	11.528179	-0.049314	4.815794
237.151532	8000.492192	11.533184	-0.049310	4.815805
237.357166	8000.476309	11.538189	-0.049349	4.815799
237.246959	8000.495877	11.543194	-0.049328	4.815806
237.308357	8000.491536	11.548199	-0.049340	4.815804
237.163997	8000.478529	11.553203	-0.049313	4.815801
237.199850	8000.497259	11.558208	-0.049319	4.815806
237.182791	8000.468165	11.563213	-0.049316	4.815798
237.161404	8000.471024	11.568218	-0.049312	4.815799
237.303619	8000.490407	11.573223	-0.049339	4.815804
237.303095	8000.460513	11.578227	-0.049339	4.815795
237.428671	8000.480695	11.583232	-0.049362	4.815800
237.451971	8000.470400	11.588237	-0.049367	4.815797
237.125652	8000.475797	11.593242	-0.049306	4.815800
237.211301	8000.473984	11.598247	-0.049322	4.815799
237.508399	8000.448906	11.603251	-0.049377	4.815791
237.401681	8000.504824	11.608256	-0.049357	4.815808
237.197117	8000.491910	11.613261	-0.049319	4.815805
237.142238	8000.475013	11.618266	-0.049309	4.815800
237.237460	8000.485096	11.623271	-0.049327	4.815803
237.231824	8000.463659	11.628275	-0.049326	4.815796
237.262306	8000.482302	11.633280	-0.049332	4.815802
237.238118	8000.484049	11.638285	-0.049327	4.815802
237.151796	8000.476250	11.643290	-0.049311	4.815800
237.267373	8000.516551	11.648295	-0.049333	4.815812
237.301492	8000.476543	11.653299	-0.049339	4.815800
237.320241	8000.471513	11.658304	-0.049343	4.815798
237.251808	8000.487487	11.663309	-0.049330	4.815803
237.338197	8000.491023	11.668314	-0.049346	4.815804
237.295048	8000.498867	11.673319	-0.049338	4.815806
237.471812	8000.452628	11.678323	-0.049371	4.815792
237.364297	8000.496792	11.683328	-0.049351	4.815805
237.583186	8000.488595	11.688333	-0.049392	4.815802
237.581154	8000.485363	11.693338	-0.049391	4.815801
237.339185	8000.500664	11.698343	-0.049346	4.815807
237.252447	8000.461903	11.703347	-0.049330	4.815796
237.401129	8000.504875	11.708352	-0.049358	4.815808
237.259168	8000.472692	11.713357	-0.049332	4.815799
237.240662	8000.483070	11.718362	-0.049328	4.815802
237.567412	8000.511844	11.723367	-0.049389	4.815809
237.337280	8000.491044	11.728371	-0.049346	4.815804
237.290275	8000.470005	11.733376	-0.049337	4.815798
237.571637	8000.494842	11.738381	-0.049390	4.815804
237.366482	8000.478716	11.743386	-0.049352	4.815800
237.611228	8000.500826	11.748391	-0.049397	4.815805
237.430761	8000.496841	11.753395	-0.049364	4.815805
237.447441	8000.521665	11.758400	-0.049367	4.815812
237.514265	8000.516345	11.763405	-0.049379	4.815810
237.526054	8000.479178	11.768410	-0.049382	4.815799
237.586460	8000.511115	11.773415	-0.049393	4.815808
237.392921	8000.477030	11.778419	-0.049357	4.815799
237.283680	8000.490209	11.783424	-0.049337	4.815804
237.310296	8000.490643	11.788429	-0.049342	4.815804
237.151839	8000.478475	11.793434	-0.049312	4.815801
237.229857	8000.501089	11.798439	-0.049327	4.815807
237.299293	8000.483002	11.803443	-0.049340	4.815802
237.323649	8000.493006	11.808448	-0.049344	4.815804
237.239991	8000.405192	11.813453	-0.049329	4.815779
237.469461	8000.495371	11.818458	-0.049371	4.815804
237.479213	8000.500869	11.823463	-0.049373	4.815806
237.545446	8000.462448	11.828467	-0.049386	4.815794
237.502229	8000.482034	11.833472	-0.049378	4.815800
237.574824	8000.474672	11.838477	-0.049391	4.815798
237.448184	8000.436332	11.843482	-0.049368	4.815787
237.586953	8000.482346	11.848487	-0.049393	4.815800
237.515847	8000.475861	11.853491	-0.049380	4.815798
237.434454	8000.504435	11.858496	-0.049365	4.815807
237.552938	8000.499951	11.863501	-0.049387	4.815805
237.458749	8000.464272	11.868506	-0.049370	4.815795
237.547710	8000.496670	11.873511	-0.049386	4.815804
237.513687	8000.471571	11.878515	-0.049380	4.815797
237.317510	8000.480142	11.883520	-0.049344	4.815801
237.544450	8000.499829	11.888525	-0.049386	4.815805
237.471170	8000.500781	11.893530	-0.049372	4.815806
237.445198	8000.511038	11.898535	-0.049367	4.815809
237.288009	8000.465799	11.903539	-0.049338	4.815797
237.499889	8000.499119	11.908544	-0.049378	4.815805
237.569561	8000.473564	11.913549	-0.049391	4.815798
237.513212	8000.487599	11.918554	-0.049380	4.815802
237.755492	8000.525682	11.923559	-0.049425	4.815812
237.647246	8000.479100	11.928563	-0.049405	4.815799
237.584561	8000.484493	11.933568	-0.049394	4.815801
237.805059	8000.488064	11.938573	-0.049435	4.815801
237.658151	8000.492094	11.943578	-0.049407	4.815803
237.535090	8000.509320	11.948583	-0.049385	4.815808
237.479436	8000.519097	11.953587	-0.049374	4.815811
237.508601	8000.517437	11.958592	-0.049380	4.815811
237.670097	8000.492300	11.963597	-0.049410	4.815803
237.486539	8000.473320	11.968602	-0.049376	4.815798
237.475360	8000.500896	11.973607	-0.049374	4.815806
237.414292	8000.456145	11.978611	-0.049362	4.815793
237.497950	8000.506605	11.983616	-0.049378	4.815808
237.585978	8000.490953	11.988621	-0.049394	4.815803
237.686855	8000.472307	11.993626	-0.049413	4.815797
237.792881	8000.486835	11.998631	-0.049433	4.815800
237.627178	8000.448931	12.003635	-0.049402	4.815790
237.658742	8000.487873	12.008640	-0.049408	4.815801
237.760056	8000.478841	12.013645	-0.049427	4.815798
237.478997	8000.494577	12.018650	-0.049375	4.815804
237.602789	8000.523269	12.023655	-0.049398	4.815812
237.500554	8000.495999	12.028659	-0.049379	4.815804
237.513761	8000.517565	12.033664	-0.049381	4.815811
237.441244	8000.509989	12.038669	-0.049368	4.815809
237.325435	8000.491039	12.043674	-0.049346	4.815804
237.468215	8000.528578	12.048679	-0.049373	4.815814
237.429945	8000.482062	12.053683	-0.049366	4.815801
237.378977	8000.492982	12.058688	-0.049356	4.815804
237.535331	8000.499785	12.063693	-0.049385	4.815805
237.523157	8000.482512	12.068698	-0.049383	4.815800
237.534815	8000.512592	12.073703	-0.049385	4.815809
237.652004	8000.503817	12.078707	-0.049407	4.815806
237.473514	8000.534022	12.083712	-0.049374	4.815816
237.623570	8000.536454	12.088717	-0.049402	4.815816
237.563320	8000.489581	12.093722	-0.049391	4.815802
237.415110	8000.521344	12.098727	-0.049363	4.815812
237.350415	8000.479737	12.103731	-0.049351	4.815800
237.629359	8000.499199	12.108736	-0.049403	4.815805
237.639388	8000.515376	12.113741	-0.049405	4.815809
237.413627	8000.383632	12.118746	-0.049363	4.815772
237.438694	8000.527078	12.123751	-0.049368	4.815814
237.672666	8000.498844	12.128755	-0.049411	4.815804
237.450254	8000.487775	12.133760	-0.049370	4.815802
237.570565	8000.492928	12.138765	-0.049392	4.815803
237.441684	8000.488710	12.143770	-0.049368	4.815803
237.473076	8000.516975	12.148775	-0.049374	4.815811
237.552212	8000.489437	12.153779	-0.049389	4.815802
237.479209	8000.516012	12.158784	-0.049376	4.815810
237.474516	8000.517007	12.163789	-0.049375	4.815811
237.500342	8000.466190	12.168794	-0.049380	4.815796
237.638770	8000.504727	12.173799	-0.049405	4.815806
237.672474	8000.478589	12.178803	-0.049412	4.815798
237.673226	8000.480739	12.183808	-0.049412	4.815799
237.577559	8000.485598	12.188813	-0.049394	4.815801
237.475429	8000.458330	12.193818	-0.049375	4.815793
237.756338	8000.530128	12.198823	-0.049427	4.815813
237.362576	8000.470386	12.203827	-0.049354	4.815798
237.394162	8000.487980	12.208832	-0.049360	4.815803
237.534899	8000.480653	12.213837	-0.049386	4.815800
237.518777	8000.483597	12.218842	-0.049383	4.815801
237.370110	8000.526027	12.223847	-0.049356	4.815814
237.640465	8000.491977	12.228851	-0.049406	4.815803
237.680026	8000.521442	12.233856	-0.049413	4.815811
237.531216	8000.514767	12.238861	-0.049386	4.815810
237.435137	8000.480124	12.243866	-0.049368	4.815800
237.676313	8000.526728	12.248871	-0.049413	4.815813
237.437252	8000.504715	12.253875	-0.049368	4.815807
237.578393	8000.509137	12.258880	-0.049395	4.815808
237.565283	8000.504658	12.263885	-0.049392	4.815807
237.393742	8000.495480	12.268890	-0.049360	4.815805
237.507377	8000.514402	12.273895	-0.049382	4.815810
237.684198	8000.489513	12.278899	-0.049415	4.815802
237.609716	8000.481905	12.283904	-0.049401	4.815800
237.606438	8000.512811	12.288909	-0.049400	4.815809
237.426443	8000.471473	12.293914	-0.049367	4.815798
237.567603	8000.530335	12.298919	-0.049393	4.815814
237.567461	8000.481233	12.303923	-0.049393	4.815800
237.595982	8000.498777	12.308928	-0.049398	4.815805
237.657642	8000.524329	12.313933	-0.049410	4.815812
237.788150	8000.497623	12.318938	-0.049434	4.815803
237.776829	8000.491038	12.323943	-0.049432	4.815802
237.543168	8000.475518	12.328947	-0.049389	4.815798
237.814261	8000.515134	12.333952	-0.049439	4.815808
237.814441	8000.523680	12.338957	-0.049439	4.815811
237.577078	8000.510234	12.343962	-0.049395	4.815808
237.693092	8000.418179	12.348967	-0.049417	4.815781
237.625078	8000.501410	12.353971	-0.049404	4.815805
237.382312	8000.504956	12.358976	-0.049359	4.815808
237.548040	8000.475617	12.363981	-0.049390	4.815798
237.412251	8000.484097	12.368986	-0.049365	4.815801
237.495636	8000.507866	12.373991	-0.049380	4.815808
237.418939	8000.489549	12.378995	-0.049366	4.815803
237.399163	8000.428388	12.384000	-0.049362	4.815785
237.295967	8000.466216	12.389005	-0.049343	4.815797
237.292131	8000.461887	12.394010	-0.049342	4.815795
237.500265	8000.487674	12.399015	-0.049381	4.815802
237.470482	8000.486128	12.404019	-0.049376	4.815802
237.469745	8000.487187	12.409024	-0.049376	4.815802
237.651072	8000.492259	12.414029	-0.049409	4.815803
237.681513	8000.470338	12.419034	-0.049415	4.815796
237.688096	8000.505673	12.424039	-0.049416	4.815806
237.583087	8000.484763	12.429043	-0.049397	4.815801
237.615658	8000.505574	12.434048	-0.049403	4.815807
237.789893	8000.515870	12.439053	-0.049435	4.815809
237.634792	8000.465327	12.444058	-0.049406	4.815795
237.709611	8000.511374	12.449063	-0.049420	4.815808
237.651981	8000.501904	12.454067	-0.049410	4.815805
237.686456	8000.494993	12.459072	-0.049416	4.815803
237.733973	8000.519249	12.464077	-0.049425	4.815810
237.504373	8000.496322	12.469082	-0.049382	4.815804
237.527258	8000.507370	12.474087	-0.049387	4.815808
237.698742	8000.465315	12.479091	-0.049419	4.815794
237.899852	8000.499529	12.484096	-0.049456	4.815803
237.911487	8000.498653	12.489101	-0.049458	4.815803
237.772224	8000.488930	12.494106	-0.049432	4.815801
237.904657	8000.526303	12.499111	-0.049457	4.815811
237.913646	8000.502967	12.504115	-0.049459	4.815804
237.784480	8000.512621	12.509120	-0.049435	4.815808
237.750477	8000.489657	12.514125	-0.049428	4.815801
237.688940	8000.488664	12.519130	-0.049417	4.815801
237.668574	8000.521429	12.524135	-0.049413	4.815811
237.673158	8000.484145	12.529139	-0.049414	4.815800
237.613463	8000.518408	12.534144	-0.049403	4.815810
237.613909	8000.518418	12.539149	-0.049403	4.815810
237.479107	8000.491688	12.544154	-0.049378	4.815803
237.849156	8000.522232	12.549159	-0.049447	4.815810
237.800277	8000.512904	12.554163	-0.049438	4.815808
237.564325	8000.522965	12.559168	-0.049394	4.815812
237.496475	8000.499453	12.564173	-0.049382	4.815805
237.548798	8000.460807	12.569178	-0.049391	4.815794
237.626041	8000.495151	12.574183	-0.049406	4.815803
237.668087	8000.473418	12.579187	-0.049414	4.815797
237.599406	8000.507535	12.584192	-0.049401	4.815807
237.618440	8000.503577	12.589197	-0.049404	4.815806
237.593575	8000.466884	12.594202	-0.049400	4.815795
237.791968	8000.513863	12.599207	-0.049437	4.815808
237.717063	8000.492372	12.604211	-0.049423	4.815802
237.601071	8000.495835	12.609216	-0.049401	4.815804
237.640292	8000.517822	12.614221	-0.049409	4.815810
237.654920	8000.470026	12.619226	-0.049411	4.815796
237.775759	8000.511481	12.624231	-0.049434	4.815808
237.716562	8000.500919	12.629235	-0.049423	4.815805
237.811570	8000.497122	12.634240	-0.049441	4.815803
238.003458	8000.434049	12.639245	-0.049476	4.815784
237.909142	8000.501910	12.644250	-0.049459	4.815804
237.911066	8000.521158	12.649255	-0.049459	4.815810
237.950028	8000.504712	12.654259	-0.049467	4.815805
237.903012	8000.494347	12.659264	-0.049458	4.815802
237.948669	8000.496157	12.664269	-0.049466	4.815802
237.867302	8000.494843	12.669274	-0.049451	4.815802
237.747515	8000.512121	12.674279	-0.049429	4.815808
237.649654	8000.499865	12.679283	-0.049411	4.815805
237.880325	8000.486523	12.684288	-0.049454	4.815800
238.013218	8000.534578	12.689293	-0.049479	4.815813
237.879310	8000.476905	12.694298	-0.049454	4.815797
237.709832	8000.507256	12.699303	-0.049422	4.815807
237.705681	8000.487978	12.704307	-0.049421	4.815801
237.692519	8000.498442	12.709312	-0.049419	4.815804
237.676607	8000.508862	12.714317	-0.049416	4.815807
237.932864	8000.475652	12.719322	-0.049464	4.815796
237.894995	8000.486784	12.724327	-0.049457	4.815800
237.823268	8000.493098	12.729331	-0.049444	4.815802
237.754868	8000.491994	12.734336	-0.049431	4.815802
238.032730	8000.483685	12.739341	-0.049483	4.815798
237.881432	8000.491913	12.744346	-0.049454	4.815801
237.758602	8000.517682	12.749351	-0.049432	4.815809
237.835149	8000.474091	12.754355	-0.049446	4.815796
237.808421	8000.468324	12.759360	-0.049441	4.815795
237.644822	8000.488096	12.764365	-0.049411	4.815801
237.857293	8000.479796	12.769370	-0.049450	4.815798
237.855684	8000.535280	12.774375	-0.049450	4.815814
237.819169	8000.511208	12.779379	-0.049443	4.815807
237.852020	8000.466910	12.784384	-0.049449	4.815794
237.846488	8000.482835	12.789389	-0.049448	4.815799
237.728322	8000.486263	12.794394	-0.049426	4.815800
237.863932	8000.506607	12.799399	-0.049452	4.815806
237.846631	8000.509533	12.804403	-0.049448	4.815807
237.841672	8000.451813	12.809408	-0.049447	4.815790
237.946590	8000.498347	12.814413	-0.049467	4.815803
237.992820	8000.486289	12.819418	-0.049476	4.815799
237.935382	8000.512048	12.824423	-0.049465	4.815807
237.906801	8000.496644	12.829427	-0.049460	4.815803
237.910030	8000.516981	12.834432	-0.049460	4.815808
238.168077	8000.511554	12.839437	-0.049508	4.815806
237.867464	8000.485342	12.844442	-0.049453	4.815799
237.987502	8000.493693	12.849447	-0.049475	4.815801
237.875375	8000.403282	12.854451	-0.049454	4.815775
237.955785	8000.498523	12.859456	-0.049469	4.815803
237.659236	8000.523614	12.864461	-0.049414	4.815812
237.725024	8000.507603	12.869466	-0.049426	4.815807
237.843082	8000.527664	12.874471	-0.049448	4.815812
237.778185	8000.521279	12.879475	-0.049436	4.815810
237.606188	8000.522768	12.884480	-0.049404	4.815812
237.719661	8000.520337	12.889485	-0.049425	4.815810
237.707629	8000.484920	12.894490	-0.049423	4.815800
237.753249	8000.497403	12.899495	-0.049432	4.815803
237.920542	8000.470225	12.904499	-0.049463	4.815795
238.018170	8000.436582	12.909504	-0.049481	4.815784
237.836315	8000.484879	12.914509	-0.049447	4.815799
237.714305	8000.441277	12.919514	-0.049424	4.815787
237.995693	8000.488533	12.924519	-0.049477	4.815800
237.845611	8000.471162	12.929523	-0.049449	4.815795
237.703040	8000.485937	12.934528	-0.049423	4.815800
237.949216	8000.488857	12.939533	-0.049468	4.815800
237.918146	8000.488357	12.944538	-0.049463	4.815800
237.774726	8000.498848	12.949543	-0.049436	4.815804
237.948789	8000.498466	12.954547	-0.049468	4.815803
237.898236	8000.480571	12.959552	-0.049459	4.815798
237.983765	8000.512915	12.964557	-0.049475	4.815807
237.643629	8000.468984	12.969562	-0.049412	4.815796
237.718627	8000.501157	12.974567	-0.049426	4.815805
237.882657	8000.500613	12.979571	-0.049456	4.815804
237.804927	8000.485480	12.984576	-0.049442	4.815800
238.016313	8000.502782	12.989581	-0.049481	4.815804
238.006522	8000.463130	12.994586	-0.049479	4.815792
238.018289	8000.514562	12.999591	-0.049482	4.815807
237.855610	8000.488448	13.004595	-0.049451	4.815800
237.855153	8000.469229	13.009600	-0.049451	4.815795
237.913172	8000.517139	13.014605	-0.049462	4.815808
237.809406	8000.478101	13.019610	-0.049443	4.815798
237.878386	8000.515515	13.024615	-0.049456	4.815808
237.976549	8000.486150	13.029619	-0.049474	4.815799
237.835224	8000.459314	13.034624	-0.049448	4.815792
237.906783	8000.508511	13.039629	-0.049461	4.815806
237.757143	8000.507159	13.044634	-0.049433	4.815806
237.782584	8000.506506	13.049639	-0.049438	4.815806
238.046798	8000.505449	13.054643	-0.049487	4.815804
238.160948	8000.519042	13.059648	-0.049509	4.815808
237.940435	8000.504801	13.064653	-0.049468	4.815805
237.770293	8000.477498	13.069658	-0.049436	4.815798
237.960007	8000.519000	13.074663	-0.049471	4.815809
237.990032	8000.503477	13.079667	-0.049477	4.815804
237.921090	8000.522646	13.084672	-0.049464	4.815810
237.907482	8000.525631	13.089677	-0.049462	4.815811
237.803833	8000.498337	13.094682	-0.049442	4.815803
237.633482	8000.523337	13.099687	-0.049411	4.815812
237.679757	8000.498470	13.104691	-0.049419	4.815804
237.937844	8000.406579	13.109696	-0.049467	4.815776
238.052747	8000.519458	13.114701	-0.049489	4.815808
237.834381	8000.490307	13.119706	-0.049448	4.815801
237.827798	8000.492338	13.124711	-0.049447	4.815802
237.975376	8000.491528	13.129715	-0.049475	4.815801
237.788170	8000.497040	13.134720	-0.049440	4.815803
237.913204	8000.530023	13.139725	-0.049463	4.815812
238.053690	8000.497074	13.144730	-0.049489	4.815802
238.018960	8000.501852	13.149735	-0.049483	4.815803
237.831447	8000.497753	13.154739	-0.049448	4.815803
237.803270	8000.456736	13.159744	-0.049443	4.815791
237.956395	8000.502983	13.164749	-0.049471	4.815804
237.749084	8000.451595	13.169754	-0.049433	4.815790
237.873912	8000.483507	13.174759	-0.049456	4.815799
237.826230	8000.491278	13.179763	-0.049447	4.815801
237.857936	8000.519548	13.184768	-0.049453	4.815809
237.881131	8000.516724	13.189773	-0.049457	4.815808
237.813621	8000.485746	13.194778	-0.049445	4.815800
237.797132	8000.511101	13.199783	-0.049442	4.815807
237.994806	8000.501494	13.204787	-0.049479	4.815803
237.997527	8000.465247	13.209792	-0.049479	4.815793
238.034876	8000.505351	13.214797	-0.049486	4.815804
237.847123	8000.479898	13.219802	-0.049451	4.815798
237.889801	8000.494469	13.224807	-0.049459	4.815802
237.946566	8000.503930	13.229811	-0.049470	4.815804
238.062203	8000.467377	13.234816	-0.049491	4.815793
238.078931	8000.500742	13.239821	-0.049495	4.815803
238.255442	8000.482253	13.244826	-0.049527	4.815797
238.056125	8000.504648	13.249831	-0.049490	4.815804
237.900467	8000.523481	13.254835	-0.049461	4.815810
237.981973	8000.462890	13.259840	-0.049477	4.815792
238.075552	8000.493230	13.264845	-0.049494	4.815801
237.995872	8000.481268	13.269850	-0.049479	4.815798
238.048153	8000.461836	13.274855	-0.049489	4.815792
238.126392	8000.481252	13.279859	-0.049504	4.815797
238.041027	8000.454254	13.284864	-0.049488	4.815789
238.058381	8000.511113	13.289869	-0.049491	4.815806
237.988274	8000.481160	13.294874	-0.049478	4.815798
237.837208	8000.475515	13.299879	-0.049450	4.815797
237.988140	8000.482231	13.304883	-0.049478	4.815798
238.027420	8000.502084	13.309888	-0.049485	4.815803
238.214514	8000.528600	13.314893	-0.049520	4.815810
238.062112	8000.478100	13.319898	-0.049492	4.815796
238.041809	8000.507663	13.324903	-0.049488	4.815805
238.168785	8000.509722	13.329907	-0.049512	4.815805
237.874408	8000.491083	13.334912	-0.049457	4.815801
238.038752	8000.505488	13.339917	-0.049488	4.815804
237.813765	8000.459151	13.344922	-0.049446	4.815792
238.039496	8000.494831	13.349927	-0.049488	4.815801
237.940917	8000.493239	13.354931	-0.049470	4.815801
237.844752	8000.490618	13.359936	-0.049452	4.815801
238.161427	8000.516028	13.364941	-0.049511	4.815807
238.024373	8000.481789	13.369946	-0.049485	4.815798
237.857671	8000.504712	13.374951	-0.049454	4.815805
237.869710	8000.493168	13.379955	-0.049457	4.815802
238.044484	8000.499203	13.384960	-0.049489	4.815803
238.219401	8000.509509	13.389965	-0.049522	4.815805
238.172433	8000.485268	13.394970	-0.049513	4.815798
238.055109	8000.510058	13.399975	-0.049491	4.815806
238.142790	8000.496536	13.404979	-0.049508	4.815801
238.144646	8000.467748	13.409984	-0.049508	4.815793
238.155645	8000.513830	13.414989	-0.049510	4.815806
237.854605	8000.489745	13.419994	-0.049454	4.815801
237.830856	8000.516050	13.424999	-0.049450	4.815808
237.818824	8000.488105	13.430003	-0.049447	4.815800
237.923319	8000.460977	13.435008	-0.049467	4.815792
237.843374	8000.509857	13.440013	-0.049452	4.815807
237.741517	8000.494334	13.445018	-0.049433	4.815803
237.957967	8000.487166	13.450023	-0.049474	4.815799
237.957925	8000.491438	13.455027	-0.049474	4.815801
237.904282	8000.488438	13.460032	-0.049464	4.815800
237.991495	8000.503730	13.465037	-0.049480	4.815804
238.074572	8000.480526	13.470042	-0.049495	4.815797
237.990585	8000.501586	13.475047	-0.049480	4.815803
238.106626	8000.514142	13.480051	-0.049501	4.815807
238.196795	8000.470771	13.485056	-0.049518	4.815793
238.119242	8000.525027	13.490061	-0.049504	4.815810
237.947225	8000.487019	13.495066	-0.049472	4.815799
238.016306	8000.503085	13.500071	-0.049485	4.815804
237.988946	8000.520792	13.505075	-0.049480	4.815809
237.799943	8000.485711	13.510080	-0.049444	4.815800
238.101034	8000.494858	13.515085	-0.049501	4.815801
238.036174	8000.477799	13.520090	-0.049489	4.815796
237.935066	8000.495380	13.525095	-0.049470	4.815802
237.983286	8000.378743	13.530099	-0.049479	4.815768
237.952707	8000.499941	13.535104	-0.049473	4.815803
237.990843	8000.502696	13.540109	-0.049480	4.815804
238.029962	8000.471309	13.545114	-0.049488	4.815794
238.122826	8000.458938	13.550119	-0.049505	4.815790
237.924059	8000.473870	13.555123	-0.049468	4.815796
237.958792	8000.482975	13.560128	-0.049474	4.815798
238.231468	8000.474582	13.565133	-0.049525	4.815794
238.183138	8000.487680	13.570138	-0.049516	4.815798
237.982946	8000.490847	13.575143	-0.049479	4.815800
238.024030	8000.496852	13.580147	-0.049487	4.815802
237.908281	8000.468295	13.585152	-0.049465	4.815794
238.009591	8000.505164	13.590157	-0.049484	4.815804
237.876848	8000.466725	13.595162	-0.049459	4.815794
237.935603	8000.423913	13.600167	-0.049470	4.815781
237.985396	8000.479163	13.605171	-0.049480	4.815797
237.992196	8000.437645	13.610176	-0.049481	4.815785
238.082497	8000.483943	13.615181	-0.049498	4.815798
238.124864	8000.467552	13.620186	-0.049506	4.815793
237.999022	8000.478328	13.625191	-0.049482	4.815797
238.073837	8000.517970	13.630195	-0.049496	4.815808
238.136088	8000.494429	13.635200	-0.049508	4.815801
238.091643	8000.505455	13.640205	-0.049500	4.815804
238.017087	8000.474362	13.645210	-0.049486	4.815795
238.258259	8000.507091	13.650215	-0.049531	4.815804
238.175368	8000.476930	13.655219	-0.049515	4.815795
238.041124	8000.425657	13.660224	-0.049490	4.815781
238.224891	8000.467063	13.665229	-0.049525	4.815792
238.285862	8000.464851	13.670234	-0.049536	4.815791
238.180585	8000.490903	13.675239	-0.049517	4.815799
237.906195	8000.480060	13.680243	-0.049465	4.815798
237.942238	8000.459297	13.685248	-0.049472	4.815791
238.089509	8000.501180	13.690253	-0.049500	4.815803
237.934397	8000.468783	13.695258	-0.049471	4.815794
238.032336	8000.466102	13.700263	-0.049489	4.815793
238.148542	8000.483998	13.705267	-0.049511	4.815798
238.150570	8000.510720	13.710272	-0.049511	4.815805
238.275256	8000.501000	13.715277	-0.049534	4.815802
238.171812	8000.474776	13.720282	-0.049515	4.815795
238.143601	8000.473255	13.725287	-0.049510	4.815794
238.212765	8000.495727	13.730291	-0.049523	4.815801
238.094976	8000.466069	13.735296	-0.049501	4.815793
238.316415	8000.523030	13.740301	-0.049542	4.815808
238.177642	8000.507977	13.745306	-0.049516	4.815804
238.118404	8000.524100	13.750311	-0.049505	4.815809
238.212817	8000.510687	13.755315	-0.049523	4.815805
237.989541	8000.492131	13.760320	-0.049482	4.815801
237.888504	8000.489431	13.765325	-0.049463	4.815800
238.040905	8000.457742	13.770330	-0.049491	4.815790
238.079029	8000.456228	13.775335	-0.049498	4.815790
238.098295	8000.475757	13.780339	-0.049502	4.815795
238.149098	8000.452030	13.785344	-0.049511	4.815788
238.143791	8000.478634	13.790349	-0.049510	4.815796
238.249548	8000.465404	13.795354	-0.049530	4.815792
238.227079	8000.507742	13.800359	-0.049526	4.815804
238.277829	8000.498960	13.805363	-0.049536	4.815801
238.105259	8000.462010	13.810368	-0.049503	4.815791
238.270995	8000.467898	13.815373	-0.049534	4.815792
238.299999	8000.437414	13.820378	-0.049540	4.815783
238.314213	8000.463267	13.825383	-0.049542	4.815791
238.066597	8000.505162	13.830387	-0.049496	4.815804
238.298973	8000.445946	13.835392	-0.049540	4.815786
238.289355	8000.469278	13.840397	-0.049538	4.815793
238.144255	8000.465865	13.845402	-0.049511	4.815792
238.220495	8000.472439	13.850407	-0.049525	4.815794
238.400381	8000.499906	13.855411	-0.049559	4.815801
238.288438	8000.499164	13.860416	-0.049538	4.815801
238.237965	8000.511160	13.865421	-0.049528	4.815805
238.295220	8000.492875	13.870426	-0.049539	4.815799
238.319077	8000.465510	13.875431	-0.049544	4.815791
238.177457	8000.470693	13.880435	-0.049517	4.815793
238.253585	8000.464456	13.885440	-0.049532	4.815791
238.434856	8000.500485	13.890445	-0.049565	4.815801
238.325499	8000.464558	13.895450	-0.049545	4.815791
238.226048	8000.480031	13.900455	-0.049526	4.815796
238.432951	8000.505800	13.905459	-0.049565	4.815803
238.322819	8000.481603	13.910464	-0.049545	4.815796
238.046267	8000.512356	13.915469	-0.049493	4.815806
238.106845	8000.465304	13.920474	-0.049504	4.815792
238.135931	8000.493531	13.925479	-0.049510	4.815800
238.117672	8000.508183	13.930483	-0.049507	4.815805
238.273139	8000.498961	13.935488	-0.049536	4.815801
238.266896	8000.515942	13.940493	-0.049534	4.815806
238.116736	8000.498570	13.945498	-0.049506	4.815802
238.072744	8000.499996	13.950503	-0.049498	4.815803
238.370344	8000.488804	13.955507	-0.049554	4.815798
238.397970	8000.470040	13.960512	-0.049559	4.815792
238.376264	8000.518795	13.965517	-0.049555	4.815807
238.273007	8000.491507	13.970522	-0.049536	4.815799
238.264314	8000.527664	13.975527	-0.049534	4.815810
238.151940	8000.515173	13.980531	-0.049513	4.815807
238.098311	8000.485486	13.985536	-0.049503	4.815798
238.246844	8000.511378	13.990541	-0.049531	4.815805
238.189611	8000.500847	13.995546	-0.049520	4.815802
238.049113	8000.484698	14.000551	-0.049494	4.815798
238.128018	8000.500923	14.005555	-0.049509	4.815803
237.987816	8000.467700	14.010560	-0.049483	4.815793
238.093210	8000.498231	14.015565	-0.049503	4.815802
238.037160	8000.486652	14.020570	-0.049492	4.815799
238.144335	8000.509739	14.025575	-0.049512	4.815805
238.119407	8000.521080	14.030579	-0.049508	4.815808
238.226862	8000.486529	14.035584	-0.049528	4.815798
238.387191	8000.495532	14.040589	-0.049557	4.815800
238.193674	8000.455041	14.045594	-0.049521	4.815789
238.157104	8000.454452	14.050599	-0.049515	4.815789
238.433477	8000.504830	14.055603	-0.049566	4.815802
238.293450	8000.443856	14.060608	-0.049540	4.815785
238.121996	8000.484849	14.065613	-0.049508	4.815798
238.282729	8000.475712	14.070618	-0.049538	4.815794
238.446803	8000.507193	14.075623	-0.049569	4.815803
238.304022	8000.432297	14.080627	-0.049542	4.815782
238.077252	8000.491609	14.085632	-0.049500	4.815800
238.042432	8000.492116	14.090637	-0.049494	4.815800
238.270217	8000.457377	14.095642	-0.049536	4.815789
238.136946	8000.457358	14.100647	-0.049511	4.815790
238.276108	8000.488435	14.105651	-0.049537	4.815798
238.283705	8000.473617	14.110656	-0.049539	4.815794
238.414555	8000.521639	14.115661	-0.049563	4.815807
238.306504	8000.501746	14.120666	-0.049543	4.815802
238.306975	8000.509229	14.125671	-0.049543	4.815804
238.236528	8000.516631	14.130675	-0.049530	4.815807
238.345331	8000.471427	14.135680	-0.049550	4.815793
238.524360	8000.534107	14.140685	-0.049584	4.815810
238.504192	8000.472937	14.145690	-0.049580	4.815793
238.472449	8000.485236	14.150695	-0.049574	4.815796
238.240674	8000.507106	14.155699	-0.049531	4.815804
238.188950	8000.457168	14.160704	-0.049521	4.815789
238.285235	8000.507833	14.165709	-0.049539	4.815804
238.134798	8000.502198	14.170714	-0.049511	4.815803
238.171544	8000.512403	14.175719	-0.049518	4.815806
238.380322	8000.533933	14.180723	-0.049557	4.815811
238.111479	8000.502897	14.185728	-0.049507	4.815803
238.149303	8000.541941	14.190733	-0.049514	4.815814
238.351614	8000.517465	14.195738	-0.049552	4.815806
238.185241	8000.483818	14.200743	-0.049521	4.815797
238.078788	8000.508785	14.205747	-0.049501	4.815805
238.106740	8000.456934	14.210752	-0.049506	4.815790
238.365689	8000.493153	14.215757	-0.049555	4.815799
238.505669	8000.477276	14.220762	-0.049581	4.815794
238.401765	8000.485204	14.225767	-0.049561	4.815797
238.256481	8000.496732	14.230771	-0.049534	4.815801
238.157592	8000.486594	14.235776	-0.049516	4.815798
238.232006	8000.528365	14.240781	-0.049530	4.815810
238.329817	8000.479781	14.245786	-0.049548	4.815795
238.322272	8000.494606	14.250791	-0.049547	4.815800
238.209974	8000.520545	14.255795	-0.049526	4.815808
238.158898	7999.372234	14.260800	-0.049516	4.815472

238.241438	7996.149287	14.265805	-0.049529	4.814529
238.286439	7990.627185	14.270810	-0.049534	4.812913
238.304561	7984.004880	14.275815	-0.049533	4.810975
238.262959	7976.669064	14.280819	-0.049520	4.808827
238.211997	7969.021035	14.285824	-0.049506	4.806586
238.150069	7961.219889	14.290829	-0.049489	4.804300
238.231776	7953.346949	14.295834	-0.049500	4.801991
237.953908	7945.377745	14.300839	-0.049443	4.799654
237.967932	7937.456161	14.305843	-0.049440	4.797329
237.956731	7929.436023	14.310848	-0.049433	4.794974
237.882104	7921.393437	14.315853	-0.049414	4.792611
237.867777	7913.405608	14.320858	-0.049406	4.790263
237.778090	7905.414296	14.325863	-0.049384	4.787913
237.915121	7897.438540	14.330867	-0.049404	4.785566
237.527906	7889.392783	14.335872	-0.049327	4.783199
237.610094	7881.419932	14.340877	-0.049337	4.780850
237.832949	7873.407277	14.345882	-0.049374	4.778488
237.538525	7865.422526	14.350887	-0.049314	4.776135
237.531241	7857.428554	14.355891	-0.049307	4.773777
237.537649	7849.362570	14.360896	-0.049303	4.771396
237.665785	7841.390911	14.365901	-0.049322	4.769042
237.441175	7833.399847	14.370906	-0.049275	4.766682
237.274914	7825.377628	14.375911	-0.049239	4.764311
237.571932	7817.433527	14.380915	-0.049289	4.761961
237.185957	7809.362970	14.385920	-0.049212	4.759575
237.097084	7801.423362	14.390925	-0.049190	4.757225
237.057956	7793.380779	14.395930	-0.049177	4.754843
237.123701	7785.352880	14.400935	-0.049184	4.752464
237.217964	7777.320870	14.405939	-0.049197	4.750083
237.034450	7769.302546	14.410944	-0.049157	4.747705
237.061479	7761.310490	14.415949	-0.049157	4.745333
236.868924	7753.352776	14.420954	-0.049116	4.742971
236.939063	7745.341847	14.425959	-0.049124	4.740591
237.014993	7737.345482	14.430963	-0.049133	4.738214
236.785548	7729.343871	14.435968	-0.049085	4.735836
236.737403	7721.325006	14.440973	-0.049071	4.733450
236.873955	7713.314014	14.445978	-0.049091	4.731065
236.746458	7705.279475	14.450983	-0.049062	4.728673
236.526806	7697.354046	14.455987	-0.049016	4.726312
236.562285	7689.283062	14.460992	-0.049018	4.723906
236.605394	7681.344966	14.465997	-0.049021	4.721538
236.382797	7673.303005	14.471002	-0.048974	4.719139
236.357652	7665.322230	14.476007	-0.048964	4.716756
236.244277	7657.339586	14.481011	-0.048938	4.714372
236.266522	7649.284793	14.486016	-0.048937	4.711964
236.347270	7641.274219	14.491021	-0.048947	4.709569
236.379699	7633.311164	14.496026	-0.048947	4.707187
236.249560	7625.260263	14.501031	-0.048918	4.704777
235.992135	7617.371080	14.506035	-0.048865	4.702415
235.903235	7609.319390	14.511040	-0.048843	4.700002
236.062757	7601.302649	14.516045	-0.048868	4.697599
236.192554	7593.305380	14.521050	-0.048887	4.695200
235.941698	7585.305659	14.526055	-0.048835	4.692800
235.910869	7577.264666	14.531059	-0.048824	4.690385
235.866227	7569.270352	14.536064	-0.048810	4.687984
235.823197	7561.294708	14.541069	-0.048797	4.685587
236.031036	7553.313098	14.546074	-0.048831	4.683186
235.889613	7545.282871	14.551079	-0.048799	4.680771
235.823951	7537.336031	14.556083	-0.048782	4.678379
235.835153	7529.314896	14.561088	-0.048779	4.675963
235.856478	7521.216129	14.566093	-0.048777	4.673522
235.627002	7513.155690	14.571098	-0.048730	4.671092
235.370606	7505.189449	14.576103	-0.048677	4.668690
235.481494	7497.227852	14.581107	-0.048692	4.666287
235.231598	7489.200727	14.586112	-0.048640	4.663863
235.179760	7481.301534	14.591117	-0.048626	4.661477
235.143780	7473.265008	14.596122	-0.048614	4.659047
234.974058	7465.243616	14.601127	-0.048577	4.656622
235.300389	7457.240362	14.606131	-0.048633	4.654200
235.197091	7449.200759	14.611136	-0.048608	4.651766
235.294695	7441.202009	14.616141	-0.048621	4.649343
235.197036	7433.242965	14.621146	-0.048598	4.646931
235.135768	7425.223334	14.626151	-0.048581	4.644499
235.118609	7417.303703	14.631155	-0.048573	4.642096
235.004637	7409.229656	14.636160	-0.048546	4.639645
234.779490	7401.279982	14.641165	-0.048499	4.637231
234.818892	7393.226058	14.646170	-0.048501	4.634784
234.494684	7385.195416	14.651175	-0.048436	4.632342
234.496993	7377.177710	14.656179	-0.048431	4.629904
234.403093	7369.207220	14.661184	-0.048408	4.627478
234.518018	7361.177555	14.666189	-0.048425	4.625033
234.386764	7353.213438	14.671194	-0.048395	4.622606
234.391086	7345.159408	14.676199	-0.048391	4.620151
234.299918	7337.217105	14.681203	-0.048369	4.617729
234.283640	7329.187978	14.686208	-0.048360	4.615278
234.232187	7321.178473	14.691213	-0.048346	4.612833
234.299871	7313.157864	14.696218	-0.048353	4.610383
234.271472	7305.148711	14.701223	-0.048342	4.607935
234.207243	7297.204081	14.706227	-0.048325	4.605505
234.158040	7289.165732	14.711232	-0.048311	4.603046
234.075231	7281.170490	14.716237	-0.048290	4.600598
234.133353	7273.217048	14.721242	-0.048296	4.598162
233.824461	7265.181828	14.726247	-0.048233	4.595699
233.978957	7257.156315	14.731251	-0.048257	4.593239
233.895206	7249.085677	14.736256	-0.048236	4.590763
233.911255	7241.132081	14.741261	-0.048234	4.588321
233.863437	7233.132059	14.746266	-0.048220	4.585864
233.655412	7225.125592	14.751271	-0.048176	4.583404
233.816472	7217.155990	14.756275	-0.048201	4.580954
233.524224	7209.088453	14.761280	-0.048141	4.578472
233.780865	7201.153476	14.766285	-0.048184	4.576030
233.510024	7193.130157	14.771290	-0.048128	4.573559
233.309866	7185.114075	14.776295	-0.048086	4.571088
233.437387	7177.183192	14.781299	-0.048104	4.568644
233.476653	7169.145554	14.786304	-0.048106	4.566164
233.444452	7161.144932	14.791309	-0.048095	4.563695
233.245351	7153.178695	14.796314	-0.048053	4.561235
233.160678	7145.154700	14.801319	-0.048032	4.558756
233.343938	7137.189382	14.806323	-0.048061	4.556294
233.142924	7129.126251	14.811328	-0.048018	4.553800
233.046170	7121.110461	14.816333	-0.047995	4.551319
233.071116	7113.077275	14.821338	-0.047995	4.548832
232.962466	7105.062312	14.826343	-0.047969	4.546348
233.041538	7097.126231	14.831347	-0.047979	4.543889
233.002248	7089.159896	14.836352	-0.047966	4.541418
232.788634	7081.148688	14.841357	-0.047921	4.538931
232.824158	7073.169553	14.846362	-0.047923	4.536454
233.059907	7065.118126	14.851367	-0.047961	4.533953
232.834425	7057.129352	14.856371	-0.047914	4.531470
232.610124	7049.057733	14.861376	-0.047867	4.528959
232.819802	7041.142101	14.866381	-0.047901	4.526497
232.907005	7033.091239	14.871386	-0.047912	4.523990
232.546826	7025.128289	14.876391	-0.047840	4.521509
232.517626	7017.138298	14.881395	-0.047829	4.519018
232.249683	7009.147589	14.886400	-0.047774	4.516526
232.475777	7001.100436	14.891405	-0.047811	4.514015
232.308264	6993.038912	14.896410	-0.047775	4.511498
232.326533	6985.027363	14.901415	-0.047773	4.508996
232.281687	6977.083716	14.906419	-0.047760	4.506513
232.115518	6969.042739	14.911424	-0.047723	4.503998
232.199375	6961.101837	14.916429	-0.047734	4.501513
232.271289	6953.062720	14.921434	-0.047742	4.498996
232.144712	6945.049867	14.926439	-0.047713	4.496486
232.052916	6937.062126	14.931443	-0.047691	4.493982
232.018715	6929.071353	14.936448	-0.047680	4.491476
231.835966	6921.066644	14.941453	-0.047640	4.488964
231.687738	6913.049246	14.946458	-0.047608	4.486446
231.751659	6905.003423	14.951463	-0.047614	4.483919
231.965429	6897.131341	14.956467	-0.047649	4.481445
231.776284	6889.090196	14.961472	-0.047609	4.478916
231.532664	6881.088986	14.966477	-0.047558	4.476397
231.779437	6873.054225	14.971482	-0.047599	4.473869
231.586507	6865.009070	14.976487	-0.047558	4.471334
231.275283	6857.063990	14.981491	-0.047494	4.468828
231.294892	6849.043428	14.986496	-0.047493	4.466299
231.296826	6841.020697	14.991501	-0.047488	4.463767
231.180952	6833.085993	14.996506	-0.047461	4.461261
230.909889	6825.036186	15.001511	-0.047406	4.458717
231.105875	6817.050437	15.006515	-0.047437	4.456194
231.064503	6809.027738	15.011520	-0.047424	4.453656
231.098134	6801.005714	15.016525	-0.047425	4.451118
231.184788	6793.051641	15.021530	-0.047436	4.448599
230.973525	6785.012399	15.026535	-0.047392	4.446052
230.930312	6777.051413	15.031539	-0.047378	4.443528
230.955828	6769.057630	15.036544	-0.047378	4.440992
230.926667	6761.019010	15.041549	-0.047367	4.438441
230.818241	6753.037251	15.046554	-0.047342	4.435906
230.666682	6744.976241	15.051559	-0.047309	4.433344
230.760085	6736.980244	15.056563	-0.047321	4.430802
230.509775	6728.974199	15.061568	-0.047269	4.428255
230.521935	6720.978793	15.066573	-0.047266	4.425710
230.597777	6712.985076	15.071578	-0.047275	4.423164
230.466733	6704.938349	15.076583	-0.047245	4.420600
230.405128	6697.007860	15.081587	-0.047229	4.418071
230.206732	6689.004826	15.086592	-0.047187	4.415517
230.439262	6680.967454	15.091597	-0.047225	4.412952
230.382925	6672.998887	15.096602	-0.047209	4.410407
230.294078	6664.954413	15.101607	-0.047187	4.407836
230.486412	6656.956936	15.106611	-0.047218	4.405279
230.405352	6649.023178	15.111616	-0.047198	4.402741
230.209656	6640.975062	15.116621	-0.047156	4.400163
230.299750	6633.026299	15.121626	-0.047168	4.397617
230.201797	6624.971393	15.126631	-0.047144	4.395035
230.190317	6616.985951	15.131635	-0.047137	4.392474
229.994242	6608.963667	15.136640	-0.047095	4.389899
229.789265	6600.999797	15.141645	-0.047052	4.387341
229.701903	6592.980269	15.146650	-0.047031	4.384764
229.682180	6585.014763	15.151655	-0.047022	4.382203
229.816472	6577.043353	15.156659	-0.047042	4.379640
229.643707	6569.045380	15.161664	-0.047004	4.377065
229.717292	6560.977812	15.166669	-0.047013	4.374467
229.826292	6552.986994	15.171674	-0.047028	4.371893
229.668066	6544.951725	15.176679	-0.046993	4.369302
229.449663	6537.028875	15.181683	-0.046947	4.366745
229.267405	6528.995963	15.186688	-0.046908	4.364151
229.499329	6521.019692	15.191693	-0.046946	4.361576
229.376266	6513.028040	15.196698	-0.046918	4.358992
229.131411	6505.050376	15.201703	-0.046867	4.356411
229.292391	6496.961311	15.206707	-0.046892	4.353795
229.308256	6488.865551	15.211712	-0.046890	4.351174
229.119788	6480.900273	15.216717	-0.046850	4.348592
229.087091	6472.966419	15.221722	-0.046838	4.346020
228.963714	6464.944879	15.226727	-0.046810	4.343418
229.074752	6457.000179	15.231731	-0.046826	4.340840
229.008876	6448.964942	15.236736	-0.046808	4.338231
228.938702	6440.975012	15.241741	-0.046790	4.335634
228.989467	6432.960393	15.246746	-0.046794	4.333029
228.680687	6424.922976	15.251751	-0.046732	4.330412
228.945419	6416.951679	15.256755	-0.046776	4.327819
228.752159	6408.918631	15.261760	-0.046735	4.325201
228.679614	6400.992198	15.266765	-0.046716	4.322618
228.854461	6392.975910	15.271770	-0.046743	4.320005
228.550597	6384.985901	15.276775	-0.046682	4.317395
228.489741	6377.013399	15.281779	-0.046665	4.314792
228.367802	6368.902908	15.286784	-0.046637	4.312141
228.451095	6360.898616	15.291789	-0.046647	4.309525
228.569657	6352.952710	15.296794	-0.046664	4.306927
228.164066	6344.895344	15.301799	-0.046584	4.304287
228.339203	6336.960624	15.306803	-0.046611	4.301690
228.234588	6328.952657	15.311808	-0.046586	4.299065
228.258573	6320.932208	15.316813	-0.046586	4.296435
227.998755	6312.977887	15.321818	-0.046532	4.293823
228.052363	6304.884782	15.326823	-0.046537	4.291167
228.191423	6296.957949	15.331827	-0.046558	4.288564
227.999350	6288.915105	15.336832	-0.046517	4.285919
227.921379	6280.937039	15.341837	-0.046497	4.283294
227.898884	6272.977653	15.346842	-0.046488	4.280674
227.773973	6264.945242	15.351847	-0.046459	4.278028
227.869977	6256.947158	15.356851	-0.046472	4.275394
227.879514	6248.885245	15.361856	-0.046468	4.272735
227.679404	6240.870782	15.366861	-0.046426	4.270090
227.591050	6232.895273	15.371866	-0.046404	4.267456
227.594598	6224.890145	15.376871	-0.046400	4.264812
227.644837	6216.935940	15.381875	-0.046404	4.262183
227.381683	6208.931923	15.386880	-0.046350	4.259533
227.329473	6200.959290	15.391885	-0.046335	4.256894
227.567719	6192.912939	15.396890	-0.046374	4.254232
227.155135	6184.899963	15.401895	-0.046292	4.251573
227.143527	6176.898851	15.406899	-0.046285	4.248920
227.179731	6168.927742	15.411904	-0.046286	4.246275
227.278008	6160.878985	15.416909	-0.046299	4.243604
227.182811	6152.979830	15.421914	-0.046277	4.240979
227.069867	6144.926505	15.426919	-0.046250	4.238301
227.036438	6136.977363	15.431923	-0.046239	4.235657
226.974046	6128.919646	15.436928	-0.046222	4.232974
226.996032	6120.893649	15.441933	-0.046221	4.230302
227.117745	6112.923163	15.446938	-0.046239	4.227647
226.952425	6104.886610	15.451943	-0.046203	4.224965
226.943009	6096.985265	15.456947	-0.046196	4.222329
227.110029	6088.944280	15.461952	-0.046222	4.219645
226.868453	6080.973031	15.466957	-0.046171	4.216980
226.744245	6072.926798	15.471962	-0.046143	4.214289
226.621844	6064.910899	15.476967	-0.046115	4.211606
226.525086	6056.978626	15.481971	-0.046092	4.208950
226.400942	6048.944170	15.486976	-0.046064	4.206257
226.556891	6040.960175	15.491981	-0.046088	4.203583
226.290562	6032.927476	15.496986	-0.046033	4.200886
226.193349	6024.968173	15.501991	-0.046009	4.198214
226.139309	6016.971716	15.506995	-0.045994	4.195528
226.062359	6008.874332	15.512000	-0.045975	4.192807
226.098210	6000.786965	15.517005	-0.045976	4.190088
226.051172	5992.870782	15.522010	-0.045962	4.187424
225.941566	5984.881981	15.527015	-0.045937	4.184733
226.055129	5976.934594	15.532019	-0.045953	4.182057
225.956790	5968.914996	15.537024	-0.045929	4.179352
225.851039	5960.924939	15.542029	-0.045904	4.176656
225.899435	5952.928475	15.547034	-0.045908	4.173957
225.941573	5944.908738	15.552039	-0.045911	4.171249
225.743645	5936.921694	15.557043	-0.045869	4.168547
225.803031	5928.876736	15.562048	-0.045875	4.165827
225.735190	5920.908681	15.567053	-0.045857	4.163129
225.405774	5912.936375	15.572058	-0.045790	4.160425
225.466281	5904.915405	15.577063	-0.045796	4.157708
225.737475	5896.924559	15.582067	-0.045842	4.155002
225.449601	5888.902231	15.587072	-0.045783	4.152276
225.363913	5880.846026	15.592077	-0.045762	4.149540
225.449720	5872.894758	15.597082	-0.045773	4.146839
225.422102	5864.871888	15.602087	-0.045762	4.144111
225.485712	5856.937295	15.607091	-0.045769	4.141412
225.366031	5848.885169	15.612096	-0.045741	4.138670
225.444915	5840.898153	15.617101	-0.045751	4.135950
225.237958	5832.901098	15.622106	-0.045707	4.133221
225.012433	5824.842390	15.627111	-0.045660	4.130470
225.032777	5816.881628	15.632115	-0.045659	4.127752
225.133943	5808.875614	15.637120	-0.045672	4.125019
224.960639	5800.927044	15.642125	-0.045635	4.122300
224.925445	5792.905654	15.647130	-0.045623	4.119556
224.810047	5784.924548	15.652135	-0.045597	4.116823
224.911206	5776.950673	15.657139	-0.045610	4.114094
224.801615	5768.875280	15.662144	-0.045585	4.111325
224.751340	5760.865920	15.667149	-0.045570	4.108577
224.641808	5752.893312	15.672154	-0.045544	4.105840
224.565232	5744.898451	15.677159	-0.045525	4.103094
224.915539	5736.924295	15.682163	-0.045585	4.100358
224.749468	5728.929971	15.687168	-0.045549	4.097607
224.538351	5720.923801	15.692173	-0.045504	4.094849
224.433661	5712.929826	15.697178	-0.045480	4.092095
224.521438	5704.894756	15.702183	-0.045491	4.089328
224.476591	5696.936422	15.707187	-0.045477	4.086584
224.373314	5688.920654	15.712192	-0.045453	4.083817
224.231926	5680.985112	15.717197	-0.045422	4.081075
224.146578	5672.996711	15.722202	-0.045401	4.078314
223.911460	5664.953905	15.727207	-0.045352	4.075530
224.017687	5656.931732	15.732211	-0.045366	4.072756
224.014281	5648.930270	15.737216	-0.045360	4.069986
223.977345	5640.905007	15.742221	-0.045348	4.067205
224.075291	5632.905817	15.747226	-0.045361	4.064433
223.811232	5624.965688	15.752231	-0.045307	4.061675
223.821113	5616.970254	15.757235	-0.045304	4.058899
223.892449	5608.954372	15.762240	-0.045312	4.056116
223.857122	5600.903549	15.767245	-0.045300	4.053317
223.739684	5592.929051	15.772250	-0.045273	4.050541
223.481377	5584.924790	15.777255	-0.045220	4.047751
223.617191	5576.952429	15.782259	-0.045240	4.044976
223.640806	5568.977743	15.787264	-0.045239	4.042196
223.347647	5560.968433	15.792269	-0.045179	4.039398
223.581159	5552.994880	15.797274	-0.045218	4.036618
223.591959	5544.901450	15.802279	-0.045214	4.033791
223.315782	5536.868124	15.807283	-0.045158	4.030979
223.110605	5528.886499	15.812288	-0.045114	4.028184
223.162328	5520.875177	15.817293	-0.045119	4.025380
223.388386	5512.905404	15.822298	-0.045156	4.022592
223.182979	5504.914738	15.827303	-0.045112	4.019788
223.160718	5496.933175	15.832307	-0.045103	4.016988
222.913254	5488.945010	15.837312	-0.045052	4.014180
222.950927	5480.913347	15.842317	-0.045054	4.011359
222.826720	5472.941661	15.847322	-0.045025	4.008555
222.910130	5464.889047	15.852327	-0.045036	4.005723
222.848446	5456.958616	15.857331	-0.045019	4.002931
222.991234	5448.932297	15.862336	-0.045040	4.000106
222.807026	5440.947806	15.867341	-0.045001	3.997288
222.694446	5432.955121	15.872346	-0.044975	3.994467
222.632551	5424.867667	15.877351	-0.044958	3.991611
222.616480	5416.936745	15.882355	-0.044950	3.988809
222.701181	5408.934330	15.887360	-0.044960	3.985981
222.293850	5400.977316	15.892365	-0.044879	3.983159
222.243447	5392.989978	15.897370	-0.044865	3.980331
222.205711	5384.976035	15.902375	-0.044853	3.977491
222.440846	5376.935565	15.907379	-0.044891	3.974644
222.175594	5368.954439	15.912384	-0.044837	3.971808
222.378817	5360.899653	15.917389	-0.044869	3.968952
222.264211	5352.984390	15.922394	-0.044843	3.966138
221.966271	5344.941415	15.927399	-0.044782	3.963273
222.097082	5336.968773	15.932403	-0.044801	3.960439
222.180544	5329.013727	15.937408	-0.044812	3.957608
222.022880	5320.990243	15.942413	-0.044777	3.954746
221.884485	5312.992703	15.947418	-0.044746	3.951892
221.906429	5304.926674	15.952423	-0.044745	3.949014
221.808782	5296.979033	15.957427	-0.044722	3.946174
221.874708	5288.974056	15.962432	-0.044729	3.943315
221.767749	5280.992172	15.967437	-0.044704	3.940459
221.845128	5273.023512	15.972442	-0.044713	3.937608
221.577378	5265.000300	15.977447	-0.044658	3.934730
221.439087	5256.995737	15.982451	-0.044627	3.931859
221.545346	5248.979541	15.987456	-0.044642	3.928985
221.444045	5241.012712	15.992461	-0.044618	3.926124
221.633639	5232.982229	15.997466	-0.044648	3.923243
221.477275	5225.006465	16.002471	-0.044613	3.920373
221.371914	5217.047017	16.007475	-0.044589	3.917508
221.203979	5209.023834	16.012480	-0.044552	3.914617
221.164951	5200.982684	16.017485	-0.044540	3.911720
221.438764	5192.969413	16.022490	-0.044586	3.908836
221.186006	5184.981516	16.027495	-0.044533	3.905949
220.920341	5177.028836	16.032499	-0.044479	3.903073
221.072441	5169.029179	16.037504	-0.044502	3.900185
220.800273	5161.017973	16.042509	-0.044446	3.897283
221.039538	5153.010041	16.047514	-0.044485	3.894390
220.676564	5144.984676	16.052519	-0.044413	3.891477
220.893449	5136.978606	16.057523	-0.044448	3.888580
220.626163	5129.002504	16.062528	-0.044393	3.885682
220.619821	5121.023672	16.067533	-0.044386	3.882786
220.704114	5113.018441	16.072538	-0.044397	3.879880
220.506916	5105.024902	16.077543	-0.044355	3.876971
220.483567	5096.980008	16.082547	-0.044346	3.874044
220.649618	5088.767192	16.087552	-0.044371	3.871057
220.523152	5080.842133	16.092557	-0.044342	3.868168
220.591627	5072.879875	16.097562	-0.044350	3.865266
220.597725	5064.969761	16.102567	-0.044346	3.862380
220.471498	5056.983958	16.107571	-0.044317	3.859462
220.234651	5049.016345	16.112576	-0.044268	3.856545
220.130379	5040.985221	16.117581	-0.044244	3.853606
220.210425	5033.018241	16.122586	-0.044253	3.850692
220.070070	5024.989470	16.127591	-0.044222	3.847749
219.972736	5017.012181	16.132595	-0.044199	3.844823
220.042715	5009.046923	16.137600	-0.044207	3.841902
219.874418	5001.045027	16.142605	-0.044170	3.838962
219.896038	4993.093810	16.147610	-0.044169	3.836041
219.738523	4985.005180	16.152615	-0.044134	3.833064
219.841716	4977.011530	16.157619	-0.044148	3.830125
219.857988	4969.031491	16.162624	-0.044146	3.827187
219.790848	4961.005624	16.167629	-0.044129	3.824228
219.938938	4953.141167	16.172634	-0.044151	3.821330
219.710003	4945.068475	16.177639	-0.044103	3.818346
219.613855	4937.096740	16.182643	-0.044080	3.815399
219.489601	4929.086411	16.187648	-0.044052	3.812436
219.476404	4921.067458	16.192653	-0.044044	3.809469
219.430730	4913.091224	16.197658	-0.044030	3.806515
219.336001	4905.125774	16.202663	-0.044008	3.803561
219.508391	4897.092750	16.207667	-0.044035	3.800587
219.376412	4889.125985	16.212672	-0.044005	3.797627
219.118610	4881.097327	16.217677	-0.043952	3.794640
219.076622	4873.093338	16.222682	-0.043939	3.791664
219.065842	4865.065270	16.227687	-0.043931	3.788677
219.053707	4857.102306	16.232691	-0.043924	3.785713
218.875981	4849.114494	16.237696	-0.043886	3.782733
218.987155	4841.086354	16.242701	-0.043901	3.779742
219.097132	4833.093035	16.247706	-0.043917	3.776762
219.013921	4825.100152	16.252711	-0.043896	3.773775
218.879271	4817.103409	16.257715	-0.043866	3.770783
218.686224	4809.114139	16.262720	-0.043824	3.767790
218.560164	4801.110533	16.267725	-0.043796	3.764791
218.782373	4793.155280	16.272730	-0.043832	3.761816
218.547746	4785.144488	16.277735	-0.043783	3.758807
218.384904	4777.163227	16.282739	-0.043748	3.755808
218.326058	4769.140420	16.287744	-0.043732	3.752794
218.461399	4761.071326	16.292749	-0.043752	3.749764
218.242919	4753.132824	16.297754	-0.043706	3.746773
218.115262	4745.106377	16.302759	-0.043677	3.743749
218.211038	4737.136232	16.307763	-0.043689	3.740748
218.323229	4729.168929	16.312768	-0.043705	3.737747
218.041162	4721.156805	16.317773	-0.043647	3.734716
218.064811	4713.172432	16.322778	-0.043647	3.731701
218.053586	4705.121591	16.327783	-0.043639	3.728658
217.997500	4697.163515	16.332787	-0.043624	3.725646
217.946467	4689.221474	16.337792	-0.043609	3.722638
217.805697	4681.168915	16.342797	-0.043578	3.719584
217.894540	4673.225951	16.347802	-0.043589	3.716574
218.042222	4665.171295	16.352807	-0.043611	3.713520
217.842183	4657.113665	16.357811	-0.043569	3.710455
217.714379	4649.129520	16.362816	-0.043540	3.707417
217.660632	4641.109430	16.367821	-0.043525	3.704364
217.526115	4633.224189	16.372826	-0.043495	3.701358
217.493644	4625.188059	16.377831	-0.043483	3.698295
217.371370	4617.233236	16.382835	-0.043455	3.695258
217.334667	4609.223783	16.387840	-0.043443	3.692199
217.479524	4601.197558	16.392845	-0.043465	3.689137
217.598284	4593.247412	16.397850	-0.043482	3.686100
217.103226	4585.219791	16.402855	-0.043385	3.683015
217.120308	4577.255430	16.407859	-0.043383	3.679965
217.204830	4569.274438	16.412864	-0.043393	3.676908
217.074985	4561.244465	16.417869	-0.043364	3.673824
216.941848	4553.241839	16.422874	-0.043334	3.670748
217.183249	4545.215049	16.427879	-0.043374	3.667670
216.935517	4537.213365	16.432883	-0.043322	3.664586
216.882628	4529.284770	16.437888	-0.043307	3.661533
216.770017	4521.241324	16.442893	-0.043281	3.658431
216.765008	4513.271068	16.447898	-0.043275	3.655358
216.738764	4505.252368	16.452903	-0.043265	3.652263
216.700234	4497.225975	16.457907	-0.043253	3.649162
216.780765	4489.247484	16.462912	-0.043263	3.646080
216.542853	4481.269440	16.467917	-0.043213	3.642987
216.468813	4473.283726	16.472922	-0.043194	3.639892
216.447098	4465.303628	16.477927	-0.043185	3.636799
216.340389	4457.295215	16.482931	-0.043160	3.633690
216.198654	4449.263999	16.487936	-0.043128	3.630568
216.255019	4441.236346	16.492941	-0.043134	3.627451
216.469840	4433.273475	16.497946	-0.043168	3.624360
216.174066	4425.322744	16.502951	-0.043108	3.621257
215.844055	4417.310885	16.507955	-0.043042	3.618127
216.024539	4409.315637	16.512960	-0.043070	3.615015
215.894519	4401.313230	16.517965	-0.043041	3.611888
215.989069	4393.311436	16.522970	-0.043053	3.608766
215.985115	4385.331538	16.527975	-0.043047	3.605646
216.057994	4377.361037	16.532979	-0.043056	3.602530
215.850504	4369.403953	16.537984	-0.043012	3.599408
215.728760	4361.417452	16.542989	-0.042984	3.596275
215.661807	4353.390270	16.547994	-0.042966	3.593124
215.370918	4345.368859	16.552999	-0.042907	3.589966
215.499427	4337.372699	16.558003	-0.042926	3.586828
215.603725	4329.400319	16.563008	-0.042940	3.583695
215.188164	4321.406936	16.568013	-0.042857	3.580537
215.242853	4313.453780	16.573018	-0.042862	3.577405
215.083246	4305.416431	16.578023	-0.042828	3.574230
215.213641	4297.398216	16.583027	-0.042847	3.571069
214.996429	4289.411843	16.588032	-0.042801	3.567908
215.101218	4281.396261	16.593037	-0.042815	3.564742
215.061911	4273.434693	16.598042	-0.042803	3.561590
214.817427	4265.452088	16.603047	-0.042752	3.558421
214.814311	4257.446163	16.608051	-0.042746	3.555246
214.919542	4249.356742	16.613056	-0.042761	3.552040
214.659445	4241.347470	16.618061	-0.042707	3.548851
214.750290	4233.393787	16.623066	-0.042719	3.545692
214.834299	4225.402181	16.628071	-0.042729	3.542514
214.779221	4217.421924	16.633075	-0.042714	3.539335
214.597893	4209.463886	16.638080	-0.042675	3.536157
214.471237	4201.465929	16.643085	-0.042646	3.532962
214.481689	4193.442197	16.648090	-0.042643	3.529758
214.480257	4185.445393	16.653095	-0.042638	3.526562
214.314129	4177.474654	16.658099	-0.042601	3.523368
214.411021	4169.522273	16.663104	-0.042614	3.520187
214.479507	4161.508366	16.668109	-0.042622	3.516977
214.405644	4153.528253	16.673114	-0.042603	3.513774
214.474638	4145.496258	16.678119	-0.042611	3.510551
214.269476	4137.521530	16.683123	-0.042567	3.507340
214.212944	4129.522519	16.688128	-0.042552	3.504120
214.183428	4121.521817	16.693133	-0.042541	3.500898
214.272865	4113.581185	16.698138	-0.042552	3.497701
214.144772	4105.559543	16.703143	-0.042523	3.494461
213.831869	4097.569913	16.708147	-0.042460	3.491225
213.880673	4089.606569	16.713152	-0.042464	3.488009
213.756076	4081.566985	16.718157	-0.042435	3.484753
213.580799	4073.635314	16.723162	-0.042398	3.481536
213.570234	4065.639522	16.728167	-0.042391	3.478295
213.920166	4057.588786	16.733171	-0.042450	3.475041
213.587878	4049.621128	16.738176	-0.042383	3.471795
213.434111	4041.580833	16.743181	-0.042350	3.468523
213.400256	4033.592334	16.748186	-0.042338	3.465272
213.420128	4025.601688	16.753191	-0.042337	3.462019
213.263438	4017.606672	16.758195	-0.042302	3.458756
213.477480	4009.623140	16.763200	-0.042337	3.455506
213.056515	4001.643159	16.768205	-0.042253	3.452234
213.010486	3993.648299	16.773210	-0.042240	3.448965
213.078569	3985.644943	16.778215	-0.042247	3.445693
213.213907	3977.647514	16.783219	-0.042267	3.442423
212.984898	3969.697161	16.788224	-0.042219	3.439157
212.973074	3961.694169	16.793229	-0.042212	3.435873
213.122022	3953.689499	16.798234	-0.042235	3.432591
212.775797	3945.669216	16.803239	-0.042165	3.429282
212.687491	3937.717569	16.808243	-0.042143	3.426008
212.756235	3929.715941	16.813248	-0.042151	3.422715
212.717910	3921.694485	16.818253	-0.042139	3.419407
212.473000	3913.781082	16.823258	-0.042088	3.416133
212.531023	3905.739973	16.828263	-0.042094	3.412813
212.543360	3897.712724	16.833267	-0.042091	3.409495
212.497295	3889.750934	16.838272	-0.042077	3.406199
212.278414	3881.754805	16.843277	-0.042031	3.402879
212.395175	3873.788175	16.848282	-0.042048	3.399579
212.537117	3865.805315	16.853287	-0.042069	3.396271
212.511094	3857.760918	16.858291	-0.042059	3.392928
212.162534	3849.741883	16.863296	-0.041989	3.389581
212.054178	3841.769873	16.868301	-0.041963	3.386258
212.094095	3833.796940	16.873306	-0.041966	3.382937
211.862364	3825.800997	16.878311	-0.041917	3.379594
211.919213	3817.852075	16.883315	-0.041923	3.376277
212.054710	3809.835550	16.888320	-0.041943	3.372932
211.799248	3801.793175	16.893325	-0.041890	3.369558
211.837767	3793.853042	16.898330	-0.041892	3.366234
211.609454	3785.887051	16.903335	-0.041844	3.362887
211.669169	3777.871619	16.908339	-0.041850	3.359526
211.752175	3769.904524	16.913344	-0.041861	3.356183
211.751254	3761.866489	16.918349	-0.041855	3.352803
211.709112	3753.865340	16.923354	-0.041842	3.349434
211.525216	3745.892710	16.928359	-0.041803	3.346068
211.674255	3737.891846	16.933363	-0.041825	3.342700
211.551182	3729.925649	16.938368	-0.041797	3.339332
211.225868	3721.960105	16.943373	-0.041732	3.335954
211.283374	3713.947152	16.948378	-0.041737	3.332567
211.224036	3705.911304	16.953383	-0.041721	3.329162
211.243280	3697.954100	16.958387	-0.041719	3.325790
211.097878	3689.990049	16.963392	-0.041687	3.322406
210.913510	3681.991344	16.968397	-0.041647	3.319001
210.935993	3674.036943	16.973402	-0.041647	3.315620
210.820978	3665.991401	16.978407	-0.041620	3.312192
210.822844	3657.973158	16.983411	-0.041615	3.308776
210.782165	3649.995522	16.988416	-0.041602	3.305372
210.609944	3642.018136	16.993421	-0.041565	3.301959
210.831163	3634.042362	16.998426	-0.041601	3.298559
210.680418	3626.055540	17.003431	-0.041568	3.295136
210.538099	3618.053021	17.008435	-0.041536	3.291704
210.561533	3610.073840	17.013440	-0.041535	3.288284
210.571302	3602.054016	17.018445	-0.041532	3.284843
210.487426	3594.138949	17.023450	-0.041511	3.281439
210.208420	3586.143161	17.028455	-0.041454	3.277989
210.233843	3578.123209	17.033459	-0.041454	3.274538
210.203059	3570.144333	17.038464	-0.041443	3.271098
210.105551	3562.130772	17.043469	-0.041419	3.267637
209.984567	3554.140179	17.048474	-0.041392	3.264181
209.917704	3546.188519	17.053479	-0.041374	3.260741
210.073774	3538.173640	17.058483	-0.041398	3.257278
210.137550	3530.165616	17.063488	-0.041405	3.253811
209.953481	3522.167358	17.068493	-0.041365	3.250335
209.914653	3514.188771	17.073498	-0.041353	3.246869
209.947875	3506.201290	17.078503	-0.041354	3.243399
209.972891	3498.223106	17.083507	-0.041353	3.239928
209.827763	3490.289331	17.088512	-0.041321	3.236467
209.546576	3482.246552	17.093517	-0.041264	3.232948
209.720426	3474.196655	17.098522	-0.041291	3.229441
209.616274	3466.224972	17.103527	-0.041266	3.225953
209.430238	3458.246101	17.108531	-0.041226	3.222455
209.287969	3450.285416	17.113536	-0.041195	3.218963
209.215893	3442.299793	17.118541	-0.041176	3.215459
209.214794	3434.312667	17.123546	-0.041171	3.211953
209.012592	3426.315629	17.128551	-0.041128	3.208431
208.917161	3418.307435	17.133555	-0.041105	3.204904
209.100816	3410.341859	17.138560	-0.041134	3.201404
209.074206	3402.345441	17.143565	-0.041124	3.197878
208.927595	3394.382722	17.148570	-0.041091	3.194357
208.883261	3386.378840	17.153575	-0.041078	3.190819
209.052779	3378.339423	17.158579	-0.041104	3.187270
209.055389	3370.388999	17.163584	-0.041100	3.183750
208.787682	3362.428278	17.168589	-0.041045	3.180210
208.910362	3354.428450	17.173594	-0.041062	3.176665
208.696646	3346.442536	17.178599	-0.041017	3.173107
208.505218	3338.424950	17.183603	-0.040977	3.169533
208.558763	3330.454457	17.188608	-0.040981	3.165986
208.347897	3322.481421	17.193613	-0.040937	3.162423
208.424298	3314.496553	17.198618	-0.040946	3.158862
208.395080	3306.519066	17.203623	-0.040935	3.155297
208.369504	3298.474225	17.208627	-0.040925	3.151697
208.374785	3290.490618	17.213632	-0.040921	3.148122
208.413755	3282.489117	17.218637	-0.040923	3.144536
208.392308	3274.533243	17.223642	-0.040914	3.140964
208.149082	3266.561719	17.228647	-0.040864	3.137372
208.071980	3258.563662	17.233651	-0.040844	3.133770
208.239014	3250.563901	17.238656	-0.040870	3.130175
207.901424	3242.598949	17.243661	-0.040802	3.126568
207.892552	3234.650867	17.248666	-0.040795	3.122980
207.851526	3226.637798	17.253671	-0.040783	3.119356
207.956314	3218.682306	17.258675	-0.040797	3.115761
207.934616	3210.682433	17.263680	-0.040788	3.112136
207.668619	3202.670890	17.268685	-0.040733	3.108491
207.639580	3194.676089	17.273690	-0.040722	3.104859
207.517952	3186.727398	17.278695	-0.040695	3.101240
207.349292	3178.731760	17.283699	-0.040658	3.097593
207.507397	3170.738070	17.288704	-0.040682	3.093958
207.334282	3162.716655	17.293709	-0.040645	3.090291
207.198477	3154.772811	17.298714	-0.040614	3.086656
207.227791	3146.767776	17.303719	-0.040615	3.082997
207.316268	3138.760779	17.308723	-0.040626	3.079335
207.276390	3130.831444	17.313728	-0.040613	3.075698
207.015321	3122.766780	17.318733	-0.040560	3.071985
207.071254	3114.772696	17.323738	-0.040565	3.068315
207.001224	3106.767791	17.328743	-0.040547	3.064629
206.916102	3098.826938	17.333747	-0.040526	3.060967
206.929134	3090.870677	17.338752	-0.040523	3.057299
206.955602	3082.859056	17.343757	-0.040523	3.053601
206.830853	3074.874048	17.348762	-0.040494	3.049904
206.677632	3066.917232	17.353767	-0.040461	3.046214
206.586961	3058.937411	17.358771	-0.040438	3.042512
206.641063	3050.946307	17.363776	-0.040443	3.038807
206.363198	3042.994661	17.368781	-0.040387	3.035100
206.285120	3035.009970	17.373786	-0.040367	3.031383
206.350597	3027.006097	17.378791	-0.040374	3.027659
206.439947	3018.985457	17.383795	-0.040385	3.023924
206.535958	3011.045504	17.388800	-0.040398	3.020222
206.355695	3003.060053	17.393805	-0.040359	3.016481
206.493631	2995.039223	17.398810	-0.040380	3.012734
206.324076	2987.067276	17.403815	-0.040343	3.008991
206.233465	2979.077740	17.408819	-0.040321	3.005238
206.135423	2971.149497	17.413824	-0.040298	3.001509
205.870050	2963.169233	17.418829	-0.040243	2.997743
206.046225	2955.155043	17.423834	-0.040271	2.993977
205.938168	2947.135331	17.428839	-0.040245	2.990191
205.688847	2939.168602	17.433843	-0.040194	2.986417
205.667026	2931.199737	17.438848	-0.040185	2.982649
205.551279	2923.210101	17.443853	-0.040158	2.978862
205.574375	2915.241531	17.448858	-0.040157	2.975087
205.468435	2907.256764	17.453863	-0.040132	2.971293
205.619502	2899.230400	17.458867	-0.040155	2.967487
205.474735	2891.283414	17.463872	-0.040123	2.963699
205.240080	2883.325552	17.468877	-0.040074	2.959896
205.236239	2875.343346	17.473882	-0.040068	2.956089
205.405525	2867.321373	17.478887	-0.040094	2.952267
205.248398	2859.339140	17.483891	-0.040060	2.948442
205.320381	2851.362720	17.488896	-0.040068	2.944626
205.140928	2843.400471	17.493901	-0.040030	2.940800
205.080232	2835.423417	17.498906	-0.040013	2.936967
205.183903	2827.427866	17.503911	-0.040027	2.933129
205.057816	2819.413352	17.508915	-0.039999	2.929265
205.077244	2811.478375	17.513920	-0.039997	2.925442
205.043772	2803.485207	17.518925	-0.039986	2.921583
204.954360	2795.531354	17.523930	-0.039964	2.917735
204.911736	2787.529381	17.528935	-0.039951	2.913861
204.566519	2779.483174	17.533939	-0.039881	2.909944
204.410904	2771.529319	17.538944	-0.039847	2.906077
204.530628	2763.531948	17.543949	-0.039864	2.902198
204.591884	2755.562580	17.548954	-0.039871	2.898324
204.383918	2747.588211	17.553959	-0.039827	2.894429
204.298986	2739.589277	17.558963	-0.039806	2.890522
204.479473	2731.604244	17.563968	-0.039834	2.886632
204.150876	2723.675142	17.568973	-0.039768	2.882736
204.153531	2715.697015	17.573978	-0.039763	2.878829
204.357187	2707.720597	17.578983	-0.039796	2.874928
204.285208	2699.688577	17.583987	-0.039777	2.870980
204.151179	2691.738685	17.588992	-0.039747	2.867063
204.196133	2683.733991	17.593997	-0.039750	2.863124
203.924850	2675.799313	17.599002	-0.039695	2.859196
203.859556	2667.833493	17.604007	-0.039677	2.855259
203.626707	2659.831382	17.609011	-0.039629	2.851289
203.799230	2651.850100	17.614016	-0.039656	2.847346
203.456781	2643.907341	17.619021	-0.039587	2.843389
203.803155	2635.907641	17.624026	-0.039646	2.839436
203.800738	2627.949165	17.629031	-0.039641	2.835478
203.345310	2619.935014	17.634035	-0.039551	2.831462
203.402939	2611.953994	17.639040	-0.039556	2.827485
203.356881	2603.949170	17.644045	-0.039542	2.823485
203.347120	2595.988988	17.649050	-0.039536	2.819504
203.313918	2588.038383	17.654055	-0.039524	2.815521
203.015314	2580.054276	17.659059	-0.039463	2.811500
203.338258	2572.030699	17.664064	-0.039518	2.807489
203.072168	2564.083234	17.669069	-0.039464	2.803477
202.927890	2556.142513	17.674074	-0.039432	2.799469
202.824348	2548.176365	17.679079	-0.039407	2.795445
202.782782	2540.156501	17.684083	-0.039394	2.791392
202.715650	2532.195682	17.689088	-0.039377	2.787361
202.611778	2524.207578	17.694093	-0.039352	2.783308
202.412686	2516.253939	17.699098	-0.039310	2.779261
202.465430	2508.272787	17.704103	-0.039315	2.775210
202.195955	2500.289411	17.709107	-0.039259	2.771132
202.492984	2492.278563	17.714112	-0.039309	2.767067
202.330706	2484.323388	17.719117	-0.039274	2.762998
202.298271	2476.351953	17.724122	-0.039263	2.758922
202.167405	2468.396579	17.729127	-0.039233	2.754843
202.190667	2460.316827	17.734131	-0.039232	2.750703
202.214688	2452.357308	17.739136	-0.039232	2.746618
201.938231	2444.403870	17.744141	-0.039175	2.742513
201.935092	2436.456793	17.749146	-0.039169	2.738421
201.978340	2428.464065	17.754151	-0.039172	2.734302
201.601149	2420.503699	17.759155	-0.039097	2.730168
201.771167	2412.515825	17.764160	-0.039123	2.726047
201.787230	2404.550451	17.769165	-0.039121	2.721921
201.696856	2396.598421	17.774170	-0.039099	2.717790
201.492385	2388.631944	17.779175	-0.039056	2.713638
201.608719	2380.603988	17.784179	-0.039072	2.709468
201.571459	2372.674981	17.789184	-0.039060	2.705333
201.268536	2364.719509	17.794189	-0.038999	2.701162
201.536623	2356.717933	17.799194	-0.039043	2.696995
201.408869	2348.753037	17.804199	-0.039015	2.692817
201.183182	2340.751721	17.809203	-0.038967	2.688607
201.108327	2332.804221	17.814208	-0.038948	2.684427
201.043597	2324.849528	17.819213	-0.038931	2.680239
201.064731	2316.887417	17.824218	-0.038930	2.676045
200.881464	2308.881028	17.829223	-0.038891	2.671808
200.984953	2300.873797	17.834227	-0.038905	2.667582
201.025869	2292.918636	17.839232	-0.038907	2.663374
200.670555	2284.969087	17.844237	-0.038836	2.659135
200.775052	2276.988533	17.849242	-0.038850	2.654904
200.663312	2269.010465	17.854247	-0.038824	2.650653
200.530003	2261.034436	17.859251	-0.038794	2.646395
200.697267	2253.058657	17.864256	-0.038820	2.642149
200.604316	2245.101639	17.869261	-0.038798	2.637890
200.549657	2237.143773	17.874266	-0.038782	2.633626
200.450947	2229.166739	17.879271	-0.038759	2.629342
200.359489	2221.187344	17.884275	-0.038737	2.625050
200.312015	2213.235029	17.889280	-0.038723	2.620768
200.195647	2205.265491	17.894285	-0.038696	2.616466
200.159837	2197.278028	17.899290	-0.038684	2.612152
199.870466	2189.342814	17.904295	-0.038625	2.607842
199.780555	2181.359175	17.909299	-0.038603	2.603513
199.908081	2173.397102	17.914304	-0.038622	2.599202
199.872363	2165.431815	17.919309	-0.038610	2.594872
199.733550	2157.258343	17.924314	-0.038579	2.590413
199.701253	2149.314804	17.929319	-0.038567	2.586080
199.567484	2141.380481	17.934323	-0.038537	2.581738
199.621535	2133.452505	17.939328	-0.038542	2.577404
199.645919	2125.471544	17.944333	-0.038542	2.573033
199.791853	2117.497039	17.949338	-0.038564	2.568665
199.653632	2109.550902	17.954343	-0.038533	2.564287
199.435056	2101.625183	17.959347	-0.038487	2.559906
199.402288	2093.696401	17.964352	-0.038476	2.555529
199.552471	2085.671936	17.969357	-0.038499	2.551105
199.320215	2077.724823	17.974362	-0.038450	2.546688
199.138664	2069.796989	17.979367	-0.038411	2.542279
198.957503	2061.828785	17.984371	-0.038372	2.537839
199.056461	2053.847559	17.989376	-0.038386	2.533404
198.986555	2045.852038	17.994381	-0.038367	2.528941
198.708523	2037.903459	17.999386	-0.038310	2.524482
198.729311	2029.972862	18.004391	-0.038309	2.520046
198.593148	2022.007636	18.009395	-0.038279	2.515572
198.835246	2013.979956	18.014400	-0.038319	2.511082
198.661045	2006.014279	18.019405	-0.038281	2.506588
198.700926	1998.048101	18.024410	-0.038283	2.502102
198.404535	1990.131334	18.029415	-0.038223	2.497611
198.558944	1982.123225	18.034419	-0.038247	2.493094
198.334670	1974.182176	18.039424	-0.038200	2.488578
198.137752	1966.228493	18.044429	-0.038158	2.484049
198.214700	1958.274409	18.049434	-0.038167	2.479532
198.170781	1950.331882	18.054439	-0.038154	2.475004
197.927216	1942.344951	18.059443	-0.038103	2.470427
197.932930	1934.383519	18.064448	-0.038099	2.465875
198.002715	1926.398998	18.069453	-0.038107	2.461306
197.812934	1918.460789	18.074458	-0.038066	2.456736
197.809320	1910.488643	18.079463	-0.038061	2.452152
197.526674	1902.537177	18.084467	-0.038003	2.447550
197.555676	1894.572825	18.089472	-0.038003	2.442956
197.434500	1886.633497	18.094477	-0.037975	2.438356
197.410057	1878.646664	18.099482	-0.037966	2.433727
197.585000	1870.606249	18.104487	-0.037993	2.429073
197.460018	1862.635273	18.109491	-0.037965	2.424428
197.481740	1854.726322	18.114496	-0.037963	2.419821
197.414629	1846.759244	18.119501	-0.037946	2.415165
197.314966	1838.800159	18.124506	-0.037922	2.410501
197.231147	1830.853624	18.129511	-0.037901	2.405838
196.908716	1822.929102	18.134515	-0.037836	2.401159
197.127675	1814.966810	18.139520	-0.037872	2.396492
197.071942	1806.993886	18.144525	-0.037856	2.391788
196.858972	1799.045569	18.149530	-0.037811	2.387076
196.954559	1791.073045	18.154535	-0.037824	2.382365
196.681496	1783.138076	18.159539	-0.037768	2.377638
196.603082	1775.196834	18.164544	-0.037748	2.372913
196.723083	1767.202841	18.169549	-0.037766	2.368163
196.616812	1759.252677	18.174554	-0.037741	2.363412
196.532216	1751.318766	18.179559	-0.037720	2.358662
196.397353	1743.363936	18.184563	-0.037689	2.353887
196.338021	1735.386527	18.189568	-0.037673	2.349094
196.265007	1727.407058	18.194573	-0.037654	2.344289
196.199197	1719.453876	18.199578	-0.037637	2.339490
196.342941	1711.498631	18.204583	-0.037659	2.334698
196.220651	1703.537074	18.209587	-0.037631	2.329870
196.276513	1695.593264	18.214592	-0.037636	2.325057
196.052264	1687.693823	18.219597	-0.037589	2.320238
196.000990	1679.745546	18.224602	-0.037574	2.315394
195.917104	1671.762170	18.229607	-0.037554	2.310516
195.880797	1663.793003	18.234611	-0.037542	2.305639
195.809530	1655.860775	18.239616	-0.037523	2.300772
195.565447	1647.928240	18.244621	-0.037473	2.295880
195.535916	1639.969297	18.249626	-0.037462	2.290980
195.609939	1631.997693	18.254631	-0.037471	2.286070
195.459062	1624.052249	18.259635	-0.037438	2.281146
195.331607	1616.140447	18.264640	-0.037409	2.276234
195.171855	1608.129442	18.269645	-0.037374	2.271248
195.263352	1600.124360	18.274650	-0.037386	2.266276
195.178713	1592.198981	18.279655	-0.037365	2.261327
195.077913	1584.253815	18.284659	-0.037341	2.256354
195.148095	1576.312880	18.289664	-0.037349	2.251387
195.016815	1568.367302	18.294669	-0.037319	2.246388
194.883972	1560.441687	18.299674	-0.037289	2.241391
194.831879	1552.514129	18.304679	-0.037274	2.236389
194.892943	1544.528527	18.309683	-0.037281	2.231349
194.927687	1536.581588	18.314688	-0.037282	2.226319
194.835063	1528.639736	18.319693	-0.037260	2.221270
194.720147	1520.708340	18.324698	-0.037233	2.216214
194.503162	1512.780617	18.329703	-0.037187	2.211140
194.654905	1504.796826	18.334707	-0.037211	2.206051
194.571665	1496.887371	18.339712	-0.037190	2.200977
194.209729	1488.984580	18.344717	-0.037117	2.195870
194.048243	1481.012695	18.349722	-0.037082	2.190725
194.162178	1473.030041	18.354727	-0.037098	2.185586
194.099684	1465.087478	18.359731	-0.037081	2.180445
193.981020	1457.167807	18.364736	-0.037054	2.175301
193.974665	1449.204160	18.369741	-0.037048	2.170127
194.206772	1441.220258	18.374746	-0.037086	2.164949
194.128650	1433.322928	18.379751	-0.037066	2.159787
193.871950	1425.409743	18.384755	-0.037013	2.154585
193.901233	1417.451164	18.389760	-0.037014	2.149367
193.743055	1409.514532	18.394765	-0.036979	2.144134
193.662331	1401.604481	18.399770	-0.036959	2.138913
193.663218	1393.660064	18.404775	-0.036954	2.133663
193.524485	1385.707004	18.409779	-0.036923	2.128382
193.373640	1377.801101	18.414784	-0.036890	2.123118
193.310834	1369.865436	18.419789	-0.036873	2.117829
193.301700	1361.890943	18.424794	-0.036866	2.112507
193.182971	1353.926280	18.429799	-0.036839	2.107166
193.054609	1345.996519	18.434803	-0.036810	2.101835
193.300217	1338.040166	18.439808	-0.036850	2.096509
193.155563	1330.109362	18.444813	-0.036818	2.091148
192.998468	1322.192718	18.449818	-0.036784	2.085782
192.996120	1314.266894	18.454823	-0.036778	2.080411
192.760047	1306.365974	18.459827	-0.036729	2.075019
192.635992	1298.441022	18.464832	-0.036701	2.069609
192.618102	1290.486889	18.469837	-0.036693	2.064175
192.862260	1282.529246	18.474842	-0.036733	2.058750
192.816289	1274.626689	18.479847	-0.036719	2.053320
192.453033	1266.704399	18.484851	-0.036646	2.047829
192.497581	1258.778052	18.489856	-0.036650	2.042363
192.432111	1250.869900	18.494861	-0.036632	2.036883
192.370230	1242.909524	18.499866	-0.036616	2.031352
192.291343	1234.976269	18.504871	-0.036596	2.025824
192.269605	1227.043760	18.509875	-0.036587	2.020286
192.078347	1219.160946	18.514880	-0.036546	2.014751
192.072640	1211.206692	18.519885	-0.036540	2.009170
192.056683	1203.272937	18.524890	-0.036532	2.003586
191.913882	1195.400434	18.529895	-0.036500	1.998017
191.571513	1187.491052	18.534899	-0.036431	1.992384
191.659732	1179.535389	18.539904	-0.036442	1.986749
191.589721	1171.614817	18.544909	-0.036424	1.981106
191.540891	1163.701887	18.549914	-0.036410	1.975454
191.630717	1155.739937	18.554919	-0.036421	1.969766
191.602606	1147.817000	18.559923	-0.036411	1.964076
191.384743	1139.953005	18.564928	-0.036365	1.958392
191.174844	1132.033064	18.569933	-0.036321	1.952652
191.321727	1124.056946	18.574938	-0.036343	1.946893
191.257834	1116.143470	18.579943	-0.036326	1.941140
191.123657	1108.232383	18.584947	-0.036296	1.935363
191.150732	1100.301920	18.589952	-0.036296	1.929573
190.988058	1092.407457	18.594957	-0.036261	1.923770
190.860470	1084.511256	18.599962	-0.036232	1.917953
190.738488	1076.614981	18.604967	-0.036204	1.912118
190.707164	1068.681721	18.609971	-0.036193	1.906249
190.629297	1060.782467	18.614976	-0.036174	1.900381
190.426214	1052.895023	18.619981	-0.036131	1.894489
190.420593	1044.949818	18.624986	-0.036124	1.888559
190.435480	1037.050982	18.629991	-0.036122	1.882647
190.230153	1029.172289	18.634995	-0.036079	1.876706
190.267351	1021.238857	18.640000	-0.036081	1.870733
190.234573	1013.301799	18.645005	-0.036069	1.864729
190.048296	1005.440490	18.650010	-0.036030	1.858747
189.980636	997.525606	18.655015	-0.036012	1.852717
190.010651	989.593553	18.660019	-0.036012	1.846667
189.917985	981.716242	18.665024	-0.035990	1.840624
189.829242	973.833203	18.670029	-0.035968	1.834557
189.685764	965.925873	18.675034	-0.035936	1.828445
189.669606	958.030687	18.680039	-0.035928	1.822337
189.388425	950.158462	18.685043	-0.035871	1.816194
189.459862	942.236784	18.690048	-0.035879	1.810034
189.280205	934.362859	18.695053	-0.035841	1.803860
189.275094	926.474066	18.700058	-0.035834	1.797675
189.286129	918.534614	18.705063	-0.035831	1.791430
189.194823	910.601573	18.710067	-0.035809	1.785156
189.435238	902.695240	18.715072	-0.035849	1.778922
189.087360	894.855594	18.720077	-0.035779	1.772646
188.968786	886.954936	18.725082	-0.035752	1.766328
189.050541	879.075872	18.730087	-0.035762	1.760029
188.817133	871.229528	18.735091	-0.035713	1.753694
188.712348	863.341357	18.740096	-0.035689	1.747319
188.601293	855.463180	18.745101	-0.035663	1.740927
188.448798	847.598625	18.750106	-0.035630	1.734518
188.372365	839.708876	18.755111	-0.035610	1.728074
188.234254	831.832573	18.760115	-0.035579	1.721610
188.389323	823.942644	18.765120	-0.035603	1.715147
188.147802	816.067845	18.770125	-0.035553	1.708621
188.008207	808.196320	18.775130	-0.035522	1.702086
188.158830	800.300648	18.780135	-0.035545	1.695543
187.998288	792.429549	18.785139	-0.035510	1.688955
188.064873	784.546794	18.790144	-0.035517	1.682362
187.654285	776.749517	18.795149	-0.035436	1.675750
187.963054	768.812551	18.800154	-0.035488	1.669091
187.767243	760.976949	18.805159	-0.035447	1.662423
187.478577	753.143575	18.810163	-0.035388	1.655718
187.636466	745.241510	18.815168	-0.035412	1.648987
187.606116	737.378076	18.820173	-0.035401	1.642236
187.393760	729.553759	18.825178	-0.035357	1.635466
187.343933	721.637342	18.830183	-0.035342	1.628611
187.108802	713.796806	18.835187	-0.035293	1.621766
187.139394	705.943403	18.840192	-0.035294	1.614919
187.158040	698.067166	18.845197	-0.035292	1.608020
187.026953	690.234876	18.850202	-0.035263	1.601110
186.770480	682.440414	18.855207	-0.035210	1.594185
186.606600	674.579836	18.860211	-0.035175	1.587184
186.885899	666.690653	18.865216	-0.035221	1.580190
186.743914	658.873205	18.870221	-0.035190	1.573169
186.605442	651.032685	18.875226	-0.035159	1.566096
186.506145	643.223219	18.880231	-0.035136	1.559025
186.335449	635.390089	18.885235	-0.035099	1.551889
186.338262	627.527738	18.890240	-0.035094	1.544720
186.255373	619.705002	18.895245	-0.035074	1.537540
186.123340	611.869953	18.900250	-0.035044	1.530308
185.993772	604.067563	18.905255	-0.035015	1.523072
185.876602	596.252365	18.910259	-0.034988	1.515792
185.784977	588.433072	18.915264	-0.034966	1.508476
185.690053	580.609446	18.920269	-0.034943	1.501121
185.426636	572.826293	18.925274	-0.034889	1.493741
185.399995	564.995918	18.930279	-0.034879	1.486316
185.290933	557.192109	18.935283	-0.034854	1.478867
185.145105	549.368617	18.940288	-0.034821	1.471355
184.988304	541.543910	18.945293	-0.034787	1.463802
185.056103	533.711326	18.950298	-0.034795	1.456237
184.970514	525.919031	18.955303	-0.034774	1.448648
184.707875	518.149424	18.960307	-0.034720	1.441012
184.948055	510.317995	18.965312	-0.034759	1.433357
184.858540	502.524437	18.970317	-0.034738	1.425644
184.572527	494.778892	18.975322	-0.034679	1.417904
184.524556	486.990969	18.980327	-0.034665	1.410119
184.447385	479.203553	18.985331	-0.034646	1.402286
184.056848	471.489718	18.990336	-0.034568	1.394431
183.717949	463.723026	18.995341	-0.034500	1.386486
183.791943	455.916673	19.000346	-0.034509	1.378525
183.587197	448.163703	19.005351	-0.034466	1.370525
183.357260	440.411240	19.010355	-0.034418	1.362475
183.279525	432.657671	19.015360	-0.034398	1.354401
182.921566	424.924923	19.020365	-0.034327	1.346252
182.783713	417.180728	19.025370	-0.034296	1.338080
182.407486	409.468882	19.030375	-0.034221	1.329849
182.319753	401.705025	19.035379	-0.034200	1.321563
182.044647	393.960801	19.040384	-0.034143	1.313212
181.835014	386.129598	19.045389	-0.034099	1.304726
181.540808	378.430621	19.050394	-0.034040	1.296312
181.533909	370.689685	19.055399	-0.034033	1.287850
180.959784	363.043786	19.060403	-0.033921	1.279332
180.556454	355.373416	19.065408	-0.033841	1.270761
180.077048	347.705501	19.070413	-0.033747	1.262120
179.618233	340.038051	19.075418	-0.033657	1.253423
179.219694	332.360954	19.080423	-0.033578	1.244667
179.004995	324.663379	19.085427	-0.033533	1.235860
178.503790	316.988650	19.090432	-0.033434	1.226960
178.082028	309.326013	19.095437	-0.033351	1.218025
177.595638	301.666182	19.100442	-0.033255	1.209014
177.257792	294.014083	19.105447	-0.033187	1.199974
176.920248	286.346816	19.110451	-0.033120	1.190847
176.564652	278.698510	19.115456	-0.033048	1.181669
176.216145	271.060901	19.120461	-0.032979	1.172432
175.781250	263.430400	19.125466	-0.032893	1.163114
175.362221	255.821733	19.130471	-0.032810	1.153749
174.806497	248.184534	19.135475	-0.032701	1.144244
174.500459	240.572398	19.140480	-0.032639	1.134743
174.061038	232.970278	19.145485	-0.032553	1.125146
173.530760	225.409458	19.150490	-0.032449	1.115498
173.190617	217.811145	19.155495	-0.032381	1.105760
172.680256	210.252251	19.160499	-0.032281	1.095948
172.046666	202.720904	19.165504	-0.032158	1.086056
171.637735	195.172496	19.170509	-0.032077	1.076101
170.987211	187.636485	19.175514	-0.031951	1.066014
170.534779	180.110078	19.180519	-0.031862	1.055888
170.139322	172.559372	19.185523	-0.031783	1.045645
169.557259	165.081915	19.190528	-0.031670	1.035356
169.141764	157.567521	19.195533	-0.031588	1.024953
168.588098	150.090679	19.200538	-0.031480	1.014461
168.639176	142.529511	19.205543	-0.031485	1.003889
167.898193	135.112282	19.210547	-0.031342	0.993213
167.471257	127.632922	19.215552	-0.031257	0.982410
167.128062	120.180452	19.220557	-0.031189	0.971547
166.589196	112.771776	19.225562	-0.031084	0.960575
166.103859	105.380038	19.230567	-0.030988	0.949515
165.587534	97.990646	19.235571	-0.030888	0.938320
165.155464	90.608618	19.240576	-0.030802	0.927023
164.655156	83.268750	19.245581	-0.030704	0.915633
164.182057	75.913575	19.250586	-0.030612	0.904083
163.721326	68.598665	19.255591	-0.030521	0.892450
162.911244	61.578421	19.260595	-0.030366	0.881037