Thu Mar 11 20:16:53 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.585195	0.109086	0.000000	0.000015	0.721401

0.725441	-0.033353	0.005005	-0.000011	0.721170
0.861606	-0.076519	0.010010	-0.000036	0.721133
0.534509	-0.022111	0.015014	0.000025	0.721126
0.657506	-0.041703	0.020019	0.000002	0.721130
0.384159	0.004006	0.025024	0.000053	0.721124
0.534196	-0.021393	0.030029	0.000025	0.721127
0.512982	-0.016931	0.035034	0.000029	0.721128
0.469678	-0.011195	0.040038	0.000037	0.721125
0.857840	-0.076339	0.045043	-0.000036	0.721132
0.669866	-0.047380	0.050048	-0.000001	0.721124
0.742108	-0.056863	0.055053	-0.000014	0.721130
0.797867	-0.066227	0.060058	-0.000025	0.721132
0.487486	-0.013368	0.065062	0.000033	0.721127
0.865990	-0.075284	0.070067	-0.000037	0.721138
0.693991	-0.059526	0.075072	-0.000005	0.721109
0.669748	-0.171278	0.080077	-0.000001	0.720880
0.585348	-0.155009	0.085082	0.000015	0.720883
0.442337	-0.132706	0.090086	0.000041	0.720877
0.619189	-0.160026	0.095091	0.000009	0.720885
0.505723	-0.142230	0.100096	0.000030	0.720880
0.663782	-0.167948	0.105101	0.000000	0.720885
0.650674	-0.238780	0.110106	0.000003	0.720741
0.386594	-0.293925	0.115110	0.000052	0.720540
0.516922	-0.311535	0.120115	0.000027	0.720551
0.437984	-0.302464	0.125120	0.000042	0.720541
0.549495	-0.321797	0.130125	0.000021	0.720542
0.465386	-0.345622	0.135130	0.000037	0.720466
0.438279	-0.463218	0.140134	0.000042	0.720225
0.507071	-0.471577	0.145139	0.000029	0.720233
0.512656	-0.476921	0.150144	0.000028	0.720224
0.393651	-0.453024	0.155149	0.000050	0.720230
0.586526	-0.636576	0.160154	0.000014	0.719936
0.740928	-0.682484	0.165158	-0.000014	0.719900
0.664022	-0.663867	0.170163	0.000000	0.719909
0.484534	-0.672333	0.175168	0.000033	0.719830
0.650260	-0.816444	0.180173	0.000003	0.719604
0.485226	-0.785539	0.185178	0.000033	0.719607
0.214671	-0.741384	0.190182	0.000084	0.719599
0.202508	-0.870439	0.195187	0.000086	0.719340
0.118471	-0.889817	0.200192	0.000102	0.719273
0.198811	-0.904868	0.205197	0.000087	0.719271
0.179846	-0.974017	0.210202	0.000090	0.719128
0.264146	-1.072580	0.215206	0.000074	0.718964
0.250116	-1.067184	0.220211	0.000077	0.718969
0.190677	-1.132417	0.225216	0.000088	0.718820
0.271131	-1.233304	0.230221	0.000073	0.718649
0.220205	-1.223355	0.235226	0.000083	0.718651
0.218819	-1.319805	0.240230	0.000083	0.718460
0.244752	-1.374498	0.245235	0.000078	0.718361
0.111728	-1.353603	0.250240	0.000103	0.718356
0.125194	-1.520302	0.255245	0.000100	0.718031
0.072980	-1.516603	0.260250	0.000110	0.718020
-0.065979	-1.554457	0.265254	0.000136	0.717897
-0.157356	-1.631143	0.270259	0.000153	0.717713
-0.087060	-1.647920	0.275264	0.000140	0.717705
-0.308193	-1.747736	0.280269	0.000181	0.717430
-0.147583	-1.797848	0.285274	0.000151	0.717387
-0.372100	-1.821194	0.290278	0.000193	0.717262
-0.404697	-1.901244	0.295283	0.000199	0.717092
-0.549364	-1.880004	0.300288	0.000226	0.717083
-0.686920	-2.016433	0.305293	0.000252	0.716765
-0.842414	-1.990343	0.310298	0.000280	0.716762
-0.717157	-2.104404	0.315302	0.000257	0.716580
-1.689537	-1.993710	0.320307	0.000438	0.716457
-1.642928	-2.006576	0.325312	0.000429	0.716448
-2.387840	-2.029700	0.330317	0.000568	0.716139
-2.584340	-1.993781	0.335322	0.000605	0.716141
-2.653602	-1.997628	0.340326	0.000618	0.716109
-3.213434	-2.008350	0.345331	0.000722	0.715890
-3.637366	-1.937155	0.350336	0.000801	0.715882
-3.594945	-1.943009	0.355341	0.000793	0.715885
-3.406249	-2.118810	0.360346	0.000758	0.715603
-4.706463	-1.915917	0.365350	0.001000	0.715546
-4.445005	-1.959847	0.370355	0.000951	0.715552
-3.980208	-2.104834	0.375360	0.000864	0.715428
-5.556977	-1.922710	0.380365	0.001158	0.715233
-5.373170	-1.951983	0.385370	0.001124	0.715240
-5.433384	-1.945497	0.390374	0.001135	0.715231
-5.136648	-2.056464	0.395379	0.001080	0.715116
-6.341045	-1.944127	0.400384	0.001304	0.714913
-6.148880	-1.977094	0.405389	0.001268	0.714916
-6.032916	-1.997154	0.410394	0.001246	0.714917
-6.369685	-1.941515	0.415398	0.001309	0.714908
-6.611321	-2.030110	0.420403	0.001354	0.714647
-7.128823	-1.957444	0.425408	0.001450	0.714609
-7.199511	-1.942955	0.430413	0.001463	0.714612
-6.671915	-2.035328	0.435418	0.001365	0.714616
-7.000992	-2.002009	0.440422	0.001426	0.714565
-7.999785	-1.963424	0.445427	0.001612	0.714289
-8.021091	-1.963549	0.450432	0.001616	0.714281
-8.258261	-1.920107	0.455437	0.001660	0.714283
-7.561031	-2.042980	0.460442	0.001531	0.714286
-8.144910	-1.945117	0.465446	0.001639	0.714274
-8.485046	-1.992942	0.470451	0.001703	0.714059
-8.958403	-1.952512	0.475456	0.001791	0.713971
-9.027737	-1.940543	0.480461	0.001803	0.713971
-9.039833	-1.936298	0.485466	0.001806	0.713975
-9.034017	-1.941253	0.490470	0.001805	0.713967
-8.857751	-1.968799	0.495475	0.001772	0.713975
-9.241337	-2.024264	0.500480	0.001843	0.713729
-10.289830	-1.873843	0.505485	0.002038	0.713657
-9.853554	-1.948502	0.510490	0.001957	0.713663
-9.773723	-1.967074	0.515494	0.001942	0.713654
-9.864980	-1.948176	0.520499	0.001959	0.713660
-9.914336	-1.940276	0.525504	0.001968	0.713658
-10.138100	-1.968545	0.530509	0.002010	0.713522
-10.784341	-1.930474	0.535514	0.002130	0.713369
-10.475268	-1.989888	0.540518	0.002073	0.713361
-10.747039	-1.936121	0.545523	0.002123	0.713371
-10.959427	-1.902352	0.550528	0.002163	0.713363
-10.750040	-1.940082	0.555533	0.002124	0.713363
-10.440519	-2.000243	0.560538	0.002066	0.713353
-11.783115	-1.927436	0.565542	0.002316	0.713022
-11.749376	-1.928458	0.570547	0.002310	0.713032
-11.536677	-1.969132	0.575552	0.002270	0.713026
-11.387285	-1.997467	0.580557	0.002242	0.713023
-11.647022	-1.947140	0.585562	0.002291	0.713031
-12.088073	-1.872704	0.590566	0.002373	0.713023
-11.499472	-2.022592	0.595571	0.002263	0.712933
-12.482556	-1.959991	0.600576	0.002446	0.712709
-12.577137	-1.941797	0.605581	0.002464	0.712712
-12.363599	-1.977288	0.610586	0.002424	0.712717
-12.384516	-1.977159	0.615590	0.002428	0.712710
-12.392939	-1.971886	0.620595	0.002429	0.712718
-12.432924	-1.967576	0.625600	0.002437	0.712712
-12.764722	-2.020276	0.630605	0.002498	0.712489
-13.700428	-1.900762	0.635610	0.002673	0.712395
-13.337254	-1.969344	0.640614	0.002605	0.712388
-13.094392	-2.008965	0.645619	0.002560	0.712395
-13.591033	-1.922384	0.650624	0.002652	0.712391
-13.517373	-1.935813	0.655629	0.002638	0.712391
-13.076813	-2.012502	0.660634	0.002556	0.712394
-14.050070	-1.969065	0.665638	0.002737	0.712136
-14.533584	-1.901624	0.670643	0.002827	0.712098
-14.308321	-1.943869	0.675648	0.002785	0.712094
-14.018245	-1.995195	0.680653	0.002731	0.712095
-14.354698	-1.933316	0.685658	0.002794	0.712099
-14.707067	-1.874359	0.690662	0.002860	0.712091
-14.218493	-1.958274	0.695667	0.002769	0.712098
-14.354289	-2.037808	0.700672	0.002794	0.711891
-15.558030	-1.885831	0.705677	0.003018	0.711766
-15.158194	-1.955269	0.710682	0.002943	0.711770
-15.172936	-1.957762	0.715686	0.002946	0.711760
-15.190651	-1.948176	0.720691	0.002949	0.711773
-14.965320	-1.991373	0.725696	0.002908	0.711767
-15.178023	-1.955420	0.730701	0.002947	0.711763
-15.432940	-2.018137	0.735706	0.002995	0.711547
-16.106645	-1.944843	0.740710	0.003120	0.711454
-16.011331	-1.956653	0.745715	0.003102	0.711465
-16.218393	-1.923152	0.750720	0.003141	0.711458
-16.639158	-1.847774	0.755725	0.003219	0.711459
-15.955117	-1.966606	0.760730	0.003092	0.711465
-16.223037	-1.922846	0.765734	0.003141	0.711457
-16.469881	-1.939146	0.770739	0.003187	0.711337
-17.363652	-1.876022	0.775744	0.003354	0.711145
-16.791154	-1.979127	0.780749	0.003247	0.711143
-17.038691	-1.931879	0.785754	0.003293	0.711149
-17.482036	-1.857130	0.790758	0.003376	0.711141
-17.036927	-1.932919	0.795763	0.003293	0.711148
-17.148832	-1.914886	0.800768	0.003314	0.711144
-17.141752	-1.917821	0.805773	0.003312	0.711141
-17.366678	-2.000561	0.810778	0.003354	0.710896
-18.062862	-1.887516	0.815782	0.003484	0.710874
-18.166122	-1.866565	0.820787	0.003503	0.710879
-17.757914	-1.940356	0.825792	0.003427	0.710877
-17.744260	-1.944774	0.830797	0.003424	0.710873
-17.722677	-1.946461	0.835802	0.003420	0.710877
-17.822885	-1.951780	0.840806	0.003439	0.710831
-18.368119	-2.000400	0.845811	0.003540	0.710540
-18.570731	-1.965770	0.850816	0.003578	0.710537
-19.030818	-1.884006	0.855821	0.003664	0.710537
-18.516156	-1.973017	0.860826	0.003568	0.710542
-18.476147	-1.986703	0.865830	0.003560	0.710529
-18.797688	-1.924548	0.870835	0.003620	0.710539
-18.828398	-1.983031	0.875840	0.003626	0.710411
-19.639869	-1.933379	0.880845	0.003777	0.710222
-19.233883	-2.003065	0.885850	0.003701	0.710227
-19.738682	-1.917158	0.890854	0.003795	0.710219
-19.689309	-1.922941	0.895859	0.003786	0.710225
-19.577703	-1.945009	0.900864	0.003765	0.710221
-19.885520	-1.891902	0.905869	0.003822	0.710218
-19.922699	-1.936939	0.910874	0.003829	0.710114
-20.813096	-1.889260	0.915878	0.003995	0.709893
-20.492164	-1.941879	0.920883	0.003935	0.709902
-20.680777	-1.910794	0.925888	0.003970	0.709897
-20.686670	-1.910634	0.930893	0.003971	0.709895
-20.517994	-1.938148	0.935898	0.003940	0.709900
-20.931077	-1.868973	0.940902	0.004017	0.709891
-20.615894	-1.921777	0.945907	0.003958	0.709898
-20.786028	-2.010423	0.950912	0.003990	0.709660
-21.762439	-1.868676	0.955917	0.004172	0.709596
-21.517925	-1.907873	0.960922	0.004126	0.709605
-21.032111	-1.999518	0.965926	0.004036	0.709595
-21.590191	-1.896811	0.970931	0.004139	0.709601
-21.676239	-1.882053	0.975936	0.004155	0.709600
-21.388497	-1.934535	0.980941	0.004102	0.709598
-21.518149	-2.040641	0.985946	0.004126	0.709339
-22.462604	-1.910226	0.990950	0.004302	0.709263
-22.470801	-1.905792	0.995955	0.004303	0.709270
-22.023312	-1.986043	1.000960	0.004220	0.709269
-22.670112	-1.873413	1.005965	0.004340	0.709263
-22.456413	-1.907043	1.010970	0.004300	0.709272
-22.228155	-1.952630	1.015974	0.004258	0.709263
-22.739220	-1.978999	1.020979	0.004353	0.709028
-23.462268	-1.885565	1.025984	0.004488	0.708957
-23.538508	-1.872827	1.030989	0.004502	0.708955
-23.119752	-1.943669	1.035994	0.004424	0.708963
-23.338341	-1.910317	1.040998	0.004465	0.708952
-23.262712	-1.920084	1.046003	0.004450	0.708959
-23.012563	-1.965477	1.051008	0.004404	0.708957
-23.492900	-1.969400	1.056013	0.004493	0.708778
-24.356823	-1.880734	1.061018	0.004654	0.708648
-23.898372	-1.966137	1.066022	0.004569	0.708640
-24.045951	-1.937214	1.071027	0.004596	0.708645
-24.572167	-1.845874	1.076032	0.004694	0.708641
-24.206257	-1.911861	1.081037	0.004626	0.708639
-23.782840	-1.983226	1.086042	0.004547	0.708647
-24.354656	-1.950387	1.091046	0.004653	0.708509
-25.267115	-1.864298	1.096051	0.004823	0.708356
-24.621317	-1.980327	1.101056	0.004703	0.708354
-25.203610	-1.878950	1.106061	0.004811	0.708349
-24.997344	-1.910135	1.111066	0.004773	0.708361
-25.076297	-1.902637	1.116070	0.004788	0.708347
-24.973444	-1.916481	1.121075	0.004768	0.708356
-25.202088	-1.932157	1.126080	0.004811	0.708243
-26.205932	-1.868019	1.131085	0.004998	0.708013
-25.757206	-1.943552	1.136090	0.004914	0.708022
-26.435211	-1.827914	1.141094	0.005040	0.708012
-26.357749	-1.839377	1.146099	0.005026	0.708017
-25.692168	-1.958311	1.151104	0.004902	0.708016
-26.146379	-1.876956	1.156109	0.004987	0.708017
-26.214103	-1.862735	1.161114	0.004999	0.708021
-26.295160	-1.952991	1.166118	0.005014	0.707812
-27.109847	-1.859728	1.171123	0.005166	0.707707
-26.946804	-1.890103	1.176128	0.005136	0.707705
-27.036629	-1.877120	1.181133	0.005152	0.707699
-26.816303	-1.912336	1.186138	0.005111	0.707707
-27.161876	-1.855168	1.191142	0.005175	0.707698
-27.138125	-1.855268	1.196147	0.005171	0.707707
-27.000090	-1.912355	1.201152	0.005145	0.707642
-27.803208	-1.900066	1.206157	0.005295	0.707379
-27.660630	-1.921698	1.211162	0.005268	0.707387
-28.137696	-1.842140	1.216166	0.005357	0.707376
-27.747726	-1.908335	1.221171	0.005284	0.707382
-27.754657	-1.908064	1.226176	0.005286	0.707381
-28.332357	-1.808000	1.231181	0.005393	0.707375
-27.740850	-1.910742	1.236186	0.005283	0.707380
-28.195009	-1.969660	1.241190	0.005368	0.707100
-28.880989	-1.854724	1.246195	0.005495	0.707085
-28.529905	-1.916752	1.251200	0.005430	0.707086
-28.451557	-1.932497	1.256205	0.005415	0.707083
-28.664007	-1.889566	1.261210	0.005455	0.707093
-28.718200	-1.884641	1.266214	0.005465	0.707083
-28.437338	-1.964126	1.271219	0.005413	0.707024
-29.697315	-1.871674	1.276224	0.005647	0.706759
-29.561726	-1.898711	1.281229	0.005622	0.706753
-29.414536	-1.919888	1.286234	0.005594	0.706764
-29.610183	-1.889124	1.291238	0.005631	0.706755
-29.828005	-1.849317	1.296243	0.005671	0.706757
-29.623944	-1.885760	1.301248	0.005633	0.706757
-29.573763	-1.895824	1.306253	0.005624	0.706755
-30.050958	-1.954270	1.311258	0.005713	0.706467
-30.808223	-1.831199	1.316262	0.005854	0.706443
-30.759494	-1.837313	1.321267	0.005844	0.706448
-30.139977	-1.946456	1.326272	0.005729	0.706451
-30.774050	-1.837848	1.331277	0.005847	0.706442
-30.404115	-1.899355	1.336282	0.005778	0.706451
-30.274266	-1.925911	1.341286	0.005754	0.706444
-30.733202	-1.970850	1.346291	0.005840	0.706190
-31.373842	-1.884595	1.351296	0.005959	0.706134
-31.538460	-1.857300	1.356301	0.005989	0.706129
-31.341510	-1.885916	1.361306	0.005953	0.706143
-31.359012	-1.888417	1.366310	0.005956	0.706131
-31.056702	-1.940397	1.371315	0.005900	0.706135
-30.923027	-1.970002	1.376320	0.005875	0.706124
-32.046536	-1.898350	1.381325	0.006084	0.705865
-31.822208	-1.934606	1.386330	0.006042	0.705873
-31.931265	-1.920784	1.391334	0.006062	0.705861
-32.142299	-1.879974	1.396339	0.006102	0.705868
-32.154882	-1.877101	1.401344	0.006104	0.705869
-32.111800	-1.886403	1.406349	0.006096	0.705866
-31.875902	-2.000080	1.411354	0.006052	0.705722
-33.505495	-1.807525	1.416358	0.006355	0.705525
-33.144642	-1.868626	1.421363	0.006288	0.705532
-32.906169	-1.911866	1.426368	0.006244	0.705530
-33.186667	-1.863600	1.431373	0.006296	0.705527
-32.870588	-1.915982	1.436378	0.006237	0.705535
-33.044170	-1.889645	1.441382	0.006269	0.705526
-33.147710	-1.916908	1.446387	0.006288	0.705434
-33.817137	-1.905477	1.451392	0.006413	0.705217
-33.898608	-1.894473	1.456397	0.006428	0.705210
-34.068163	-1.859276	1.461402	0.006460	0.705220
-33.966490	-1.882084	1.466406	0.006441	0.705210
-33.708857	-1.924941	1.471411	0.006393	0.705216
-34.039573	-1.867837	1.476416	0.006454	0.705213
-34.248764	-1.855697	1.481421	0.006493	0.705162
-34.350851	-1.970552	1.486426	0.006512	0.704894
-34.231399	-1.996141	1.491430	0.006490	0.704886
-34.718032	-1.906045	1.496435	0.006581	0.704893
-34.772892	-1.895714	1.501440	0.006591	0.704894
-34.554666	-1.937478	1.506445	0.006550	0.704888
-34.434534	-1.954391	1.511450	0.006528	0.704897
-34.964336	-1.979036	1.516454	0.006626	0.704657
-35.730838	-1.873328	1.521459	0.006769	0.704595
-35.511111	-1.909549	1.526464	0.006728	0.704601
-35.461469	-1.922613	1.531469	0.006719	0.704593
-35.460726	-1.918979	1.536474	0.006719	0.704600
-35.440098	-1.925941	1.541478	0.006715	0.704594
-35.578981	-1.908688	1.546483	0.006740	0.704579
-36.348507	-1.925846	1.551488	0.006884	0.704268
-36.479153	-1.906030	1.556493	0.006908	0.704261
-36.567779	-1.884685	1.561498	0.006924	0.704272
-36.656476	-1.872155	1.566502	0.006941	0.704265
-36.366495	-1.923226	1.571507	0.006887	0.704267
-36.254749	-1.944185	1.576512	0.006866	0.704265
-36.633307	-1.879513	1.581517	0.006937	0.704259
-36.863421	-1.968306	1.586522	0.006979	0.703997
-37.198771	-1.929601	1.591526	0.007042	0.703955
-37.547059	-1.864324	1.596531	0.007107	0.703961
-37.605279	-1.855987	1.601536	0.007117	0.703957
-37.811660	-1.821312	1.606541	0.007156	0.703953
-37.440701	-1.883494	1.611546	0.007087	0.703961
-37.497510	-1.877692	1.616550	0.007097	0.703952
-37.829579	-1.893545	1.621555	0.007159	0.703801
-38.417930	-1.866087	1.626560	0.007269	0.703645
-37.929565	-1.957637	1.631565	0.007178	0.703636
-38.205748	-1.904287	1.636570	0.007229	0.703644
-38.255316	-1.899658	1.641574	0.007238	0.703636
-38.220823	-1.903749	1.646579	0.007232	0.703640
-38.104075	-1.924866	1.651584	0.007210	0.703640
-38.477243	-1.953464	1.656589	0.007279	0.703448
-39.065919	-1.897064	1.661594	0.007389	0.703350
-39.024980	-1.907835	1.666598	0.007381	0.703343
-38.963269	-1.916509	1.671603	0.007370	0.703347
-38.767187	-1.950843	1.676608	0.007333	0.703349
-38.990453	-1.915165	1.681613	0.007375	0.703341
-39.025625	-1.913409	1.686618	0.007381	0.703331
-39.460593	-1.999582	1.691622	0.007462	0.703001
-39.718134	-1.949790	1.696627	0.007510	0.703009
-39.996370	-1.897738	1.701632	0.007562	0.703014
-40.281110	-1.851096	1.706637	0.007615	0.703006
-39.564887	-1.972916	1.711642	0.007482	0.703017
-39.911562	-1.918400	1.716646	0.007546	0.703003
-40.180534	-1.911896	1.721651	0.007596	0.702919
-40.689555	-1.930845	1.726656	0.007691	0.702698
-40.780431	-1.919616	1.731661	0.007708	0.702688
-40.911080	-1.891484	1.736666	0.007732	0.702697
-40.872188	-1.902235	1.741670	0.007725	0.702690
-40.913605	-1.893838	1.746675	0.007733	0.702692
-40.793791	-1.912682	1.751680	0.007710	0.702697
-40.813512	-1.934379	1.756685	0.007714	0.702646
-41.138672	-2.009463	1.761690	0.007774	0.702377
-41.607417	-1.929001	1.766694	0.007862	0.702371
-42.146549	-1.831048	1.771699	0.007962	0.702375
-41.676332	-1.914497	1.776704	0.007874	0.702376
-41.683366	-1.916670	1.781709	0.007876	0.702369
-41.988559	-1.858384	1.786714	0.007932	0.702377
-41.731436	-1.916499	1.791718	0.007885	0.702352
-42.377904	-1.937780	1.796723	0.008005	0.702076
-42.622886	-1.891774	1.801728	0.008050	0.702081
-43.023487	-1.823113	1.806733	0.008125	0.702075
-42.287160	-1.951699	1.811738	0.007988	0.702081
-42.242811	-1.963457	1.816742	0.007980	0.702073
-42.765159	-1.869422	1.821747	0.008077	0.702075
-42.575294	-1.919244	1.826752	0.008041	0.702042
-43.187240	-1.958033	1.831757	0.008155	0.701743
-43.260167	-1.942360	1.836762	0.008169	0.701749
-43.853046	-1.838484	1.841766	0.008279	0.701745
-43.339277	-1.929394	1.846771	0.008184	0.701747
-43.200257	-1.952517	1.851776	0.008158	0.701750
-43.711787	-1.866464	1.856781	0.008253	0.701740
-43.234629	-1.983206	1.861786	0.008164	0.701676
-44.096930	-1.949050	1.866790	0.008325	0.701434
-44.192373	-1.929863	1.871795	0.008342	0.701438
-44.107379	-1.943122	1.876800	0.008326	0.701442
-44.334947	-1.907045	1.881805	0.008369	0.701433
-44.287440	-1.909957	1.886810	0.008360	0.701444
-44.324842	-1.905477	1.891814	0.008367	0.701440
-44.236342	-1.988597	1.896819	0.008350	0.701304
-45.342021	-1.878987	1.901824	0.008556	0.701126
-45.345682	-1.881294	1.906829	0.008557	0.701120
-44.791257	-1.975836	1.911834	0.008454	0.701129
-44.942304	-1.953363	1.916838	0.008482	0.701120
-45.230676	-1.899389	1.921843	0.008535	0.701125
-45.148553	-1.912137	1.926848	0.008520	0.701129
-45.409920	-1.935032	1.931853	0.008569	0.700989
-45.932996	-1.894025	1.936858	0.008666	0.700883
-45.755223	-1.929262	1.941862	0.008633	0.700876
-45.812414	-1.918169	1.946867	0.008643	0.700878
-45.777735	-1.923768	1.951872	0.008637	0.700879
-46.052428	-1.878126	1.956877	0.008688	0.700872
-45.797738	-1.920416	1.961882	0.008641	0.700879
-46.392693	-1.982992	1.966886	0.008751	0.700537
-46.879639	-1.896147	1.971891	0.008842	0.700537
-46.842585	-1.902747	1.976896	0.008835	0.700537
-46.699267	-1.931069	1.981901	0.008808	0.700531
-47.019931	-1.868641	1.986906	0.008868	0.700542
-46.961396	-1.882383	1.991910	0.008857	0.700535
-46.604450	-1.963200	1.996915	0.008791	0.700501
-47.649069	-1.915430	2.001920	0.008985	0.700220

-47.519019	-1.937913	2.011917	0.008961	0.700221
-47.760718	-1.893484	2.021914	0.009006	0.700224
-47.590790	-1.923386	2.031910	0.008974	0.700225
-47.796277	-1.888151	2.041907	0.009012	0.700222
-47.680420	-1.910067	2.051904	0.008991	0.700220
-47.658245	-1.912965	2.061901	0.008986	0.700222
-47.807548	-1.885514	2.071898	0.009014	0.700224
-47.742678	-1.898647	2.081894	0.009002	0.700221
-47.778152	-1.890879	2.091891	0.009008	0.700224
-47.900929	-1.868967	2.101888	0.009031	0.700224
-47.792630	-1.888265	2.111885	0.009011	0.700224
-47.828377	-1.871739	2.121882	0.009018	0.700245
-46.974582	-1.879293	2.131878	0.008859	0.700539
-46.948650	-1.885675	2.141875	0.008854	0.700535
-46.839270	-1.904741	2.151872	0.008833	0.700536
-46.789675	-1.913492	2.161869	0.008824	0.700537
-47.053147	-1.865103	2.171866	0.008873	0.700539
-46.092462	-1.884671	2.181862	0.008694	0.700847
-46.141444	-1.862151	2.191859	0.008703	0.700875
-45.782937	-1.925024	2.201856	0.008636	0.700877
-46.010040	-1.883970	2.211853	0.008679	0.700879
-45.776700	-1.863768	2.221850	0.008635	0.701004
-45.227750	-1.904041	2.231846	0.008533	0.701121
-45.492886	-1.856243	2.241843	0.008582	0.701122
-45.358439	-1.881552	2.251840	0.008557	0.701120
-44.439010	-1.897408	2.261837	0.008386	0.701420
-44.559092	-1.865904	2.271834	0.008408	0.701440
-44.254423	-1.920177	2.281830	0.008351	0.701440
-44.569375	-1.825317	2.291827	0.008410	0.701519
-43.578489	-1.890089	2.301824	0.008225	0.701745
-43.632877	-1.880027	2.311821	0.008235	0.701746
-43.493182	-1.905693	2.321818	0.008209	0.701745
-42.951480	-1.870625	2.331814	0.008108	0.702011
-42.869646	-1.855874	2.341811	0.008093	0.702071
-42.609146	-1.902501	2.351808	0.008044	0.702071
-42.682134	-1.840666	2.361805	0.008058	0.702169
-41.929114	-1.875897	2.371802	0.007918	0.702370
-41.914885	-1.878495	2.381798	0.007915	0.702370
-42.014741	-1.862336	2.391795	0.007933	0.702367
-41.115217	-1.870098	2.401792	0.007766	0.702675
-41.190010	-1.848083	2.411789	0.007780	0.702693
-40.802093	-1.916885	2.421786	0.007707	0.702694
-40.886668	-1.825165	2.431782	0.007723	0.702849
-40.104196	-1.887596	2.441779	0.007577	0.703005
-40.021826	-1.901609	2.451776	0.007562	0.703006
-39.822343	-1.936309	2.461773	0.007525	0.703008
-39.440134	-1.873940	2.471770	0.007454	0.703272
-39.179223	-1.886184	2.481766	0.007405	0.703341
-39.345321	-1.857095	2.491763	0.007436	0.703340
-39.012624	-1.875437	2.501760	0.007374	0.703423
-38.442704	-1.870970	2.511757	0.007268	0.703637
-38.179708	-1.919431	2.521754	0.007219	0.703634
-38.582140	-1.848013	2.531750	0.007293	0.703633
-37.559063	-1.894240	2.541747	0.007103	0.703908
-37.493138	-1.884551	2.551744	0.007090	0.703952
-37.501565	-1.883768	2.561741	0.007092	0.703950
-37.263756	-1.881587	2.571738	0.007048	0.704040
-36.604304	-1.889879	2.581734	0.006925	0.704261
-36.715355	-1.871925	2.591731	0.006945	0.704257
-36.436130	-1.919984	2.601728	0.006893	0.704261
-35.983487	-1.873878	2.611725	0.006809	0.704517
-35.541831	-1.914283	2.621722	0.006727	0.704594
-35.817851	-1.867424	2.631718	0.006778	0.704589
-35.602348	-1.874604	2.641715	0.006738	0.704652
-35.032630	-1.859073	2.651712	0.006632	0.704888
-34.805505	-1.899509	2.661709	0.006589	0.704889
-34.818359	-1.895920	2.671706	0.006592	0.704891
-34.413557	-1.833750	2.681702	0.006516	0.705162
-34.100273	-1.865981	2.691699	0.006458	0.705210
-33.676381	-1.941572	2.701696	0.006379	0.705210
-33.909398	-1.843760	2.711693	0.006422	0.705323
-32.831829	-1.935458	2.721690	0.006222	0.705525
-33.147527	-1.880367	2.731686	0.006280	0.705523
-33.069555	-1.893900	2.741683	0.006266	0.705524
-32.629265	-1.829807	2.751680	0.006184	0.705811
-32.123759	-1.893209	2.761677	0.006089	0.705865
-32.005499	-1.914119	2.771674	0.006067	0.705865
-32.276225	-1.822784	2.781670	0.006118	0.705952
-31.363365	-1.897071	2.791667	0.005948	0.706130
-31.525089	-1.867875	2.801664	0.005978	0.706131
-31.446794	-1.882126	2.811661	0.005963	0.706130
-30.807154	-1.840681	2.821658	0.005844	0.706443
-30.497842	-1.895023	2.831654	0.005786	0.706445
-30.425881	-1.908534	2.841651	0.005773	0.706443
-30.308458	-1.841893	2.851648	0.005751	0.706619
-29.367681	-1.941800	2.861645	0.005576	0.706756
-29.594229	-1.900778	2.871642	0.005618	0.706757
-29.549293	-1.909705	2.881638	0.005609	0.706755
-28.840548	-1.878636	2.891635	0.005477	0.707072
-28.958501	-1.850432	2.901632	0.005499	0.707086
-28.486219	-1.934131	2.911629	0.005411	0.707087
-28.639558	-1.831058	2.921626	0.005440	0.707239
-27.901831	-1.891743	2.931622	0.005302	0.707382
-27.896943	-1.892831	2.941619	0.005301	0.707381
-27.858894	-1.892742	2.951616	0.005294	0.707395
-26.916762	-1.906586	2.961613	0.005119	0.707704
-27.035411	-1.886317	2.971610	0.005141	0.707703
-26.982793	-1.896224	2.981606	0.005131	0.707702
-26.847181	-1.836246	2.991603	0.005105	0.707871
-26.277721	-1.864333	3.001600	0.004999	0.708018
-26.084525	-1.899726	3.011597	0.004963	0.708016
-26.207992	-1.843786	3.021594	0.004986	0.708084
-24.888799	-1.945693	3.031590	0.004741	0.708352
-25.216479	-1.887546	3.041587	0.004801	0.708351
-25.209350	-1.887746	3.051584	0.004800	0.708353
-24.977952	-1.863872	3.061581	0.004757	0.708484
-24.408417	-1.884918	3.071578	0.004651	0.708645
-24.441829	-1.879921	3.081574	0.004657	0.708643
-24.421448	-1.874328	3.091571	0.004653	0.708662
-23.743505	-1.846444	3.101568	0.004527	0.708960
-23.249216	-1.931242	3.111565	0.004435	0.708967
-23.637452	-1.862110	3.121562	0.004507	0.708967
-23.001570	-1.881526	3.131558	0.004388	0.709155
-22.783815	-1.863382	3.141555	0.004348	0.709269
-22.616288	-1.890917	3.151552	0.004317	0.709274
-22.631787	-1.862087	3.161549	0.004319	0.709326
-21.797036	-1.871844	3.171546	0.004164	0.709604
-21.482163	-1.928802	3.181542	0.004105	0.709603
-21.704622	-1.889960	3.191539	0.004147	0.709601
-21.344796	-1.885567	3.201536	0.004080	0.709738
-20.465474	-1.959668	3.211533	0.003916	0.709904
-21.001391	-1.863714	3.221530	0.004015	0.709905
-20.802045	-1.901451	3.231526	0.003978	0.709900
-20.435862	-1.825624	3.241523	0.003910	0.710182
-19.921765	-1.896301	3.251520	0.003814	0.710224
-19.900884	-1.898714	3.261517	0.003810	0.710227
-19.636516	-1.876462	3.271514	0.003761	0.710366
-19.006673	-1.901835	3.281510	0.003644	0.710539
-19.021361	-1.899630	3.291507	0.003646	0.710539
-19.110422	-1.883781	3.301504	0.003663	0.710539
-18.513988	-1.833505	3.311501	0.003552	0.710852
-18.144896	-1.885246	3.321498	0.003483	0.710880
-18.048083	-1.903616	3.331494	0.003465	0.710878
-18.219005	-1.823655	3.341491	0.003497	0.710977
-17.263321	-1.910221	3.351488	0.003319	0.711144
-17.428327	-1.880409	3.361485	0.003349	0.711145
-17.279871	-1.904887	3.371482	0.003322	0.711149
-16.813012	-1.832160	3.381478	0.003235	0.711460
-16.615061	-1.868121	3.391475	0.003198	0.711459
-16.499803	-1.888094	3.401472	0.003176	0.711460
-16.101814	-1.852447	3.411469	0.003102	0.711673
-15.660489	-1.882192	3.421466	0.003020	0.711770
-15.538689	-1.903839	3.431462	0.002997	0.711770
-15.674974	-1.852685	3.441459	0.003022	0.711824
-14.697149	-1.890299	3.451456	0.002840	0.712097
-14.780893	-1.874300	3.461453	0.002856	0.712099
-14.859142	-1.860222	3.471450	0.002870	0.712099
-14.479916	-1.812930	3.481446	0.002799	0.712328
-14.123728	-1.844601	3.491443	0.002733	0.712392
-13.960542	-1.873424	3.501440	0.002703	0.712392
-13.853753	-1.813997	3.511437	0.002683	0.712549
-12.871002	-1.905604	3.521434	0.002500	0.712715
-12.814425	-1.915157	3.531430	0.002489	0.712716
-12.856371	-1.906567	3.541427	0.002497	0.712719
-12.228305	-1.893647	3.551424	0.002380	0.712967
-11.832543	-1.931236	3.561421	0.002306	0.713033
-11.717437	-1.953338	3.571418	0.002285	0.713030
-11.863241	-1.928009	3.581414	0.002312	0.713029
-11.292219	-1.890762	3.591411	0.002205	0.713305
-11.147604	-1.886022	3.601408	0.002178	0.713366
-10.930993	-1.922594	3.611405	0.002138	0.713370
-10.836186	-1.929528	3.621402	0.002120	0.713390
-10.339206	-1.883650	3.631398	0.002028	0.713658
-10.041066	-1.938717	3.641395	0.001972	0.713654
-9.936554	-1.956808	3.651392	0.001953	0.713655
-9.927929	-1.904590	3.661389	0.001951	0.713762
-8.926797	-1.975870	3.671386	0.001764	0.713975
-9.167627	-1.933889	3.681382	0.001809	0.713973
-9.245865	-1.921072	3.691379	0.001824	0.713971
-8.670136	-1.921837	3.701376	0.001716	0.714174
-8.256841	-1.940729	3.711373	0.001639	0.714282
-7.978805	-1.989577	3.721370	0.001588	0.714284
-8.119489	-1.965833	3.731366	0.001614	0.714281
-7.352394	-1.958410	3.741363	0.001471	0.714568
-7.486451	-1.913529	3.751360	0.001496	0.714609
-7.122972	-1.975590	3.761357	0.001428	0.714615
-7.299106	-1.912190	3.771354	0.001461	0.714679
-6.359110	-1.960569	3.781350	0.001286	0.714915
-6.516613	-1.935366	3.791347	0.001315	0.714910
-6.510005	-1.936014	3.801344	0.001314	0.714911
-5.911618	-1.942716	3.811341	0.001202	0.715109
-5.329364	-1.982250	3.821338	0.001094	0.715237
-5.877510	-1.883439	3.831334	0.001196	0.715239
-5.396019	-1.964982	3.841331	0.001106	0.715247
-4.964645	-1.889695	3.851328	0.001025	0.715549
-4.562910	-1.958996	3.861325	0.000951	0.715554
-4.737777	-1.928418	3.871322	0.000983	0.715553
-4.218244	-1.919673	3.881318	0.000886	0.715754
-3.778476	-1.930684	3.891315	0.000804	0.715887
-3.610814	-1.960494	3.901312	0.000773	0.715888
-3.566490	-1.967859	3.911309	0.000765	0.715889
-3.066934	-1.950453	3.921306	0.000672	0.716100
-2.943635	-1.953818	3.931302	0.000649	0.716137
-2.793932	-1.981611	3.941299	0.000621	0.716135
-2.823986	-1.928659	3.951296	0.000626	0.716229
-2.189479	-1.927383	3.961293	0.000508	0.716455
-1.960014	-1.968871	3.971290	0.000465	0.716454
-2.129988	-1.939010	3.981286	0.000497	0.716454
-1.761809	-1.857324	3.991283	0.000428	0.716745
-1.444269	-1.906406	4.001280	0.000369	0.716760
-1.573144	-1.882721	4.011277	0.000393	0.716762
-1.376915	-1.766469	4.021274	0.000356	0.717061
-1.644668	-1.703707	4.031270	0.000406	0.717091
-1.220468	-1.715402	4.041267	0.000327	0.717217
-1.033773	-1.665376	4.051264	0.000292	0.717382
-1.151337	-1.621337	4.061261	0.000314	0.717428
-0.857418	-1.531000	4.071258	0.000259	0.717710
-0.800799	-1.542016	4.081254	0.000248	0.717709
-0.647671	-1.412304	4.091251	0.000220	0.718019
-0.936171	-1.341557	4.101248	0.000273	0.718057
-0.767932	-1.218735	4.111245	0.000242	0.718359
-0.585242	-1.192718	4.121242	0.000208	0.718475
-0.536694	-1.113186	4.131238	0.000199	0.718649
-0.763410	-0.950114	4.141235	0.000241	0.718891
-0.256371	-0.963518	4.151232	0.000146	0.719043
-0.519918	-0.801149	4.161229	0.000195	0.719271
-0.111455	-0.735356	4.171226	0.000119	0.719544
-0.293314	-0.608591	4.181222	0.000153	0.719730
-0.261206	-0.508723	4.191219	0.000147	0.719939
-0.287197	-0.356222	4.201216	0.000151	0.720230
-0.152509	-0.240333	4.211213	0.000126	0.720506
-0.033549	-0.127902	4.221210	0.000104	0.720769
-0.100682	0.005084	4.231206	0.000116	0.721007
0.000000	0.133881	4.241203	0.000097	0.721296

0.044203	0.767131	4.246208	0.000089	0.722556
0.247266	2.003767	4.251213	0.000050	0.725050
0.643159	3.794357	4.256218	-0.000025	0.728682
1.182114	6.122277	4.261222	-0.000127	0.733385
1.367819	9.010735	4.266227	-0.000163	0.739014
1.640645	12.371522	4.271232	-0.000216	0.745529
2.208170	16.132478	4.276237	-0.000325	0.752841
2.303427	20.379290	4.281242	-0.000345	0.760832
2.874220	24.945951	4.286246	-0.000454	0.769486
3.635301	29.839940	4.291251	-0.000599	0.778701
3.999796	35.164403	4.296256	-0.000671	0.788456
4.620456	40.758894	4.301261	-0.000790	0.798651
5.279712	46.642633	4.306266	-0.000917	0.809238
6.191971	52.782968	4.311270	-0.001091	0.820208
6.654676	59.266679	4.316275	-0.001181	0.831483
7.325737	65.944014	4.321280	-0.001310	0.842995
8.035514	72.840076	4.326285	-0.001447	0.854726
9.032641	79.885631	4.331290	-0.001637	0.866625
9.795293	87.179936	4.336294	-0.001784	0.878698
10.503705	94.643697	4.341299	-0.001921	0.890860
11.320587	102.264724	4.346304	-0.002078	0.903136
11.821340	110.081477	4.351309	-0.002176	0.915464
12.470505	117.974698	4.356314	-0.002302	0.927784
13.041521	126.018959	4.361318	-0.002414	0.940149
13.483857	134.168299	4.366323	-0.002502	0.952477
14.109045	142.381815	4.371328	-0.002623	0.964788
14.991036	150.636561	4.376333	-0.002793	0.977069
15.572817	159.026090	4.381338	-0.002907	0.989314
15.994485	167.492699	4.386342	-0.002991	1.001479
16.488501	175.970117	4.391347	-0.003089	1.013531
17.200299	184.463332	4.396352	-0.003227	1.025515
17.507156	193.060780	4.401357	-0.003289	1.037407
18.032828	201.630633	4.406362	-0.003393	1.049177
19.044547	210.169410	4.411366	-0.003587	1.060888
19.838767	218.753463	4.416371	-0.003740	1.072480
20.448265	227.374461	4.421376	-0.003860	1.083954
21.527988	235.936836	4.426381	-0.004066	1.095337
22.173024	244.567972	4.431386	-0.004192	1.106594
22.804306	253.234591	4.436390	-0.004315	1.117780
23.488415	261.858676	4.441395	-0.004448	1.128812
24.161566	270.505409	4.446400	-0.004579	1.139764
24.841140	279.166692	4.451405	-0.004711	1.150629
25.416167	287.809992	4.456410	-0.004824	1.161349
26.318130	296.386100	4.461414	-0.004998	1.171957
26.717525	305.024271	4.466419	-0.005078	1.182441
27.485843	313.608657	4.471424	-0.005226	1.192844
28.076624	322.199962	4.476429	-0.005342	1.203128
28.525243	330.810006	4.481434	-0.005431	1.213319
29.011037	339.402254	4.486438	-0.005527	1.223411
29.179369	348.038906	4.491443	-0.005564	1.233410
30.205674	356.499262	4.496448	-0.005761	1.243293
30.948576	365.013628	4.501453	-0.005905	1.253104
31.318864	373.553966	4.506458	-0.005979	1.262797
31.919666	382.077860	4.511462	-0.006097	1.272441
32.447807	390.553795	4.516467	-0.006201	1.281946
33.098389	399.029142	4.521472	-0.006327	1.291403
33.747164	407.484427	4.526477	-0.006454	1.300768
34.348086	415.994692	4.531482	-0.006571	1.310117
34.685456	424.549904	4.536486	-0.006640	1.319400
35.114641	432.967408	4.541491	-0.006725	1.328488
35.638504	441.380389	4.546496	-0.006828	1.337525
36.038122	449.782631	4.551501	-0.006908	1.346469
36.477107	458.192371	4.556506	-0.006995	1.355368
37.026101	466.564714	4.561510	-0.007103	1.364189
37.366457	474.966742	4.566515	-0.007172	1.372948
37.702684	483.348560	4.571520	-0.007240	1.381630
38.357791	491.698751	4.576525	-0.007368	1.390279
38.707482	500.062524	4.581530	-0.007438	1.398837
39.042440	508.425383	4.586534	-0.007506	1.407339
39.190114	516.800988	4.591539	-0.007539	1.415772
39.578210	525.118715	4.596544	-0.007617	1.424137
40.236192	533.421085	4.601549	-0.007745	1.432481
40.400569	541.764413	4.606554	-0.007781	1.440738
40.955297	550.057492	4.611558	-0.007889	1.448961
41.280565	558.375422	4.616563	-0.007955	1.457124
41.546987	566.689017	4.621568	-0.008010	1.465229
42.024089	575.025237	4.626573	-0.008105	1.473344
42.176005	583.328245	4.631578	-0.008139	1.481331
42.670300	591.582095	4.636582	-0.008236	1.489282
42.876520	599.882167	4.641587	-0.008280	1.497190
43.445423	608.110886	4.646592	-0.008391	1.505045
44.100937	616.357934	4.651597	-0.008519	1.512889
44.411792	624.606800	4.656602	-0.008582	1.520642
45.061740	632.828930	4.661606	-0.008708	1.528382
45.285111	641.117550	4.666611	-0.008755	1.536080
45.692961	649.359146	4.671616	-0.008837	1.543724
46.039664	657.622494	4.676621	-0.008907	1.551340
46.429170	665.852340	4.681626	-0.008985	1.558896
46.899135	674.070114	4.686630	-0.009077	1.566415
47.162380	682.321139	4.691635	-0.009132	1.573898
47.713471	690.521138	4.696640	-0.009240	1.581342
48.127442	698.753326	4.701645	-0.009322	1.588760
48.423315	706.990938	4.706650	-0.009383	1.596130
48.718061	715.217386	4.711654	-0.009443	1.603457
49.117917	723.418136	4.716659	-0.009523	1.610743
49.570190	731.627801	4.721664	-0.009613	1.618011
50.077605	739.816693	4.726669	-0.009712	1.625236
50.474588	748.073608	4.731674	-0.009792	1.632472
50.695592	756.307580	4.736678	-0.009838	1.639632
50.964151	764.483159	4.741683	-0.009894	1.646717
51.269222	772.693035	4.746688	-0.009956	1.653807
51.762062	780.849541	4.751693	-0.010053	1.660845
52.158566	789.018118	4.756698	-0.010132	1.667851
52.579502	797.223177	4.761702	-0.010216	1.674862
52.967277	805.383668	4.766707	-0.010293	1.681802
53.238965	813.575663	4.771712	-0.010349	1.688723
53.550450	821.782791	4.776717	-0.010413	1.695635
53.838457	829.955810	4.781722	-0.010472	1.702486
54.388162	838.124419	4.786726	-0.010579	1.709341
54.626328	846.325175	4.791731	-0.010629	1.716154
55.102658	854.457936	4.796736	-0.010723	1.722915
55.660110	862.601469	4.801741	-0.010832	1.729669
55.867789	870.805512	4.806746	-0.010876	1.736401
56.398927	878.943711	4.811750	-0.010981	1.743094
56.581179	887.136918	4.816755	-0.011020	1.749762
56.950902	895.308108	4.821760	-0.011094	1.756411
57.313522	903.451925	4.826765	-0.011167	1.763011
57.634515	911.604865	4.831770	-0.011232	1.769589
58.392726	919.719841	4.836774	-0.011379	1.776166
58.488849	927.905147	4.841779	-0.011402	1.782693
58.894134	936.065871	4.846784	-0.011483	1.789214
59.277729	944.269661	4.851789	-0.011559	1.795743
59.240174	952.449757	4.856794	-0.011558	1.802179
59.903194	960.523613	4.861798	-0.011687	1.808593
60.189074	968.682855	4.866803	-0.011745	1.815005
60.612345	976.799265	4.871808	-0.011829	1.821378
61.033948	984.938342	4.876813	-0.011913	1.827746
61.204136	993.117428	4.881818	-0.011950	1.834093
61.660777	1001.229888	4.886822	-0.012041	1.840400
62.041999	1009.349232	4.891827	-0.012117	1.846682
62.309230	1017.511221	4.896832	-0.012172	1.852962
62.813788	1025.636762	4.901837	-0.012271	1.859221
62.946677	1033.786755	4.906842	-0.012301	1.865434
63.189912	1041.968880	4.911846	-0.012352	1.871663
63.625804	1050.064468	4.916851	-0.012438	1.877828
63.977422	1058.177281	4.921856	-0.012509	1.883976
64.337308	1066.309847	4.926861	-0.012582	1.890120
64.445395	1074.455636	4.931866	-0.012607	1.896226
65.073095	1082.537431	4.936870	-0.012729	1.902322
65.173010	1090.697515	4.941875	-0.012753	1.908398
65.629557	1098.823841	4.946880	-0.012844	1.914469
66.125837	1106.908141	4.951885	-0.012941	1.920495
66.476468	1115.007140	4.956890	-0.013012	1.926496
66.645929	1123.190987	4.961894	-0.013049	1.932521
66.945296	1131.308970	4.966899	-0.013110	1.938492
67.310330	1139.413457	4.971904	-0.013183	1.944443
67.663724	1147.567004	4.976909	-0.013254	1.950410
67.974210	1155.711519	4.981914	-0.013317	1.956348
68.564579	1163.772305	4.986918	-0.013433	1.962237
68.764365	1171.875450	4.991923	-0.013475	1.968097
69.075287	1180.006143	4.996928	-0.013538	1.973971
69.682450	1188.064546	5.001933	-0.013657	1.979807
69.846226	1196.186599	5.006938	-0.013693	1.985625
70.249523	1204.304023	5.011942	-0.013773	1.991447
70.333301	1212.439742	5.016947	-0.013794	1.997232
70.643744	1220.527303	5.021952	-0.013857	2.002989
70.939252	1228.628665	5.026957	-0.013917	2.008738
71.345918	1236.730610	5.031962	-0.013998	2.014483
71.684435	1244.832695	5.036966	-0.014067	2.020204
71.937499	1252.929108	5.041971	-0.014119	2.025896
72.411824	1261.041667	5.046976	-0.014213	2.031606
72.935098	1269.136331	5.051981	-0.014315	2.037293
72.971518	1277.248805	5.056986	-0.014328	2.042926
73.305624	1285.351765	5.061990	-0.014395	2.048568
73.392662	1293.489561	5.066995	-0.014417	2.054193
73.832511	1301.553127	5.072000	-0.014504	2.059787
74.423562	1309.609815	5.077005	-0.014619	2.065376
74.807473	1317.712207	5.082010	-0.014696	2.070960
75.244541	1325.832932	5.087014	-0.014783	2.076548
75.339105	1333.924059	5.092019	-0.014806	2.082066
75.648607	1342.011240	5.097024	-0.014869	2.087587
75.961014	1350.144137	5.102029	-0.014932	2.093126
76.373671	1358.201449	5.107034	-0.015014	2.098608
76.611112	1366.308098	5.112038	-0.015064	2.104093
76.653950	1374.456335	5.117043	-0.015077	2.109572
76.956697	1382.602027	5.122048	-0.015139	2.115060
77.469259	1390.630362	5.127053	-0.015239	2.120476
77.786131	1398.686952	5.132058	-0.015304	2.125877
78.167613	1406.772155	5.137062	-0.015380	2.131291
78.288090	1414.882963	5.142067	-0.015408	2.136682
78.566679	1422.954831	5.147072	-0.015465	2.142049
79.014562	1431.034047	5.152077	-0.015554	2.147424
79.240571	1439.130225	5.157082	-0.015601	2.152775
79.438219	1447.243647	5.162086	-0.015643	2.158122
79.874202	1455.283462	5.167091	-0.015730	2.163429
80.253995	1463.357105	5.172096	-0.015806	2.168740
80.532050	1471.471308	5.177101	-0.015863	2.174055
80.589925	1479.578709	5.182106	-0.015879	2.179333
80.880563	1487.654965	5.187110	-0.015938	2.184598
81.345339	1495.726020	5.192115	-0.016030	2.189864
81.625222	1503.830672	5.197120	-0.016087	2.195122
82.173102	1511.871243	5.202125	-0.016195	2.200350
82.289407	1519.944326	5.207130	-0.016222	2.205547
82.460169	1528.053993	5.212134	-0.016259	2.210760
82.898443	1536.122325	5.217139	-0.016346	2.215959
83.374207	1544.167922	5.222144	-0.016440	2.221135
83.782769	1552.246491	5.227149	-0.016521	2.226313
83.757772	1560.370718	5.232154	-0.016522	2.231469
84.316748	1568.425852	5.237158	-0.016631	2.236622
84.426004	1576.514599	5.242163	-0.016657	2.241744
84.661953	1584.581460	5.247168	-0.016706	2.246852
85.157511	1592.664467	5.252173	-0.016803	2.251981
85.452350	1600.732454	5.257178	-0.016864	2.257071
85.600336	1608.826057	5.262182	-0.016896	2.262153
86.151859	1616.866232	5.267187	-0.017004	2.267225
86.576289	1625.005085	5.272192	-0.017089	2.272336
86.923353	1633.103444	5.277197	-0.017159	2.277404
86.850485	1641.167591	5.282202	-0.017150	2.282403
87.249554	1649.209502	5.287206	-0.017230	2.287418
87.596258	1657.272013	5.292211	-0.017300	2.292430
87.842180	1665.341453	5.297216	-0.017351	2.297427
88.085511	1673.408173	5.302221	-0.017402	2.302411
88.468834	1681.452222	5.307226	-0.017478	2.307382
88.732990	1689.557003	5.312230	-0.017533	2.312369
89.091426	1697.608040	5.317235	-0.017605	2.317321
89.362923	1705.668193	5.322240	-0.017661	2.322260
89.702193	1713.740311	5.327245	-0.017729	2.327202
89.786205	1721.842729	5.332250	-0.017750	2.332130
90.277723	1729.891722	5.337254	-0.017847	2.337049
90.586906	1737.948162	5.342259	-0.017910	2.341948
90.720815	1746.033034	5.347264	-0.017940	2.346839
91.308242	1754.110818	5.352269	-0.018055	2.351752
91.529211	1762.180062	5.357274	-0.018101	2.356620
91.915660	1770.219579	5.362278	-0.018178	2.361473
92.110565	1778.300949	5.367283	-0.018220	2.366326
92.495281	1786.358584	5.372288	-0.018297	2.371170
92.935820	1794.438306	5.377293	-0.018384	2.376022
92.923760	1802.503936	5.382298	-0.018387	2.380819
93.344677	1810.559380	5.387302	-0.018471	2.385635
93.507635	1818.654845	5.392307	-0.018506	2.390445
93.996378	1826.703106	5.397312	-0.018603	2.395242
94.430826	1834.749134	5.402317	-0.018689	2.400025
94.775783	1842.781513	5.407322	-0.018758	2.404782
95.131748	1850.851700	5.412326	-0.018830	2.409553
95.267543	1858.957260	5.417331	-0.018861	2.414319
95.427710	1867.017783	5.422336	-0.018896	2.419050
95.778664	1875.075076	5.427341	-0.018966	2.423785
96.015813	1883.152702	5.432346	-0.019016	2.428514
96.298697	1891.277246	5.437350	-0.019074	2.433264
96.630080	1899.316240	5.442355	-0.019141	2.437959
96.845973	1907.342234	5.447360	-0.019186	2.442629
97.051732	1915.411802	5.452365	-0.019230	2.447314
97.478665	1923.441690	5.457370	-0.019314	2.451984
98.022956	1931.486151	5.462374	-0.019421	2.456662
98.307952	1939.542502	5.467379	-0.019479	2.461318
98.427832	1947.614118	5.472384	-0.019507	2.465962
99.019948	1955.665841	5.477389	-0.019623	2.470621
99.100367	1963.750678	5.482394	-0.019643	2.475252
99.317952	1971.800578	5.487398	-0.019689	2.479865
99.634202	1979.847858	5.492403	-0.019753	2.484475
99.890634	1987.908443	5.497408	-0.019806	2.489079
99.935146	1996.023686	5.502413	-0.019819	2.493690
100.264310	2004.041632	5.507418	-0.019886	2.498259
100.686892	2012.077595	5.512422	-0.019970	2.502836
100.950094	2020.142735	5.517427	-0.020024	2.507409
100.938579	2028.262306	5.522432	-0.020027	2.511985
101.633834	2036.290820	5.527437	-0.020162	2.516552
101.885772	2044.303082	5.532442	-0.020214	2.521070
102.176899	2052.357468	5.537446	-0.020274	2.525606
102.447226	2060.415227	5.542451	-0.020329	2.530135
102.551910	2068.505969	5.547456	-0.020354	2.534661
102.684397	2076.574077	5.552461	-0.020384	2.539169
102.957981	2084.590076	5.557466	-0.020440	2.543650
103.256815	2092.675104	5.562470	-0.020501	2.548164
103.400812	2100.738830	5.567475	-0.020533	2.552646
103.602668	2108.778449	5.572480	-0.020576	2.557111
104.217525	2116.813036	5.577485	-0.020696	2.561595
104.273298	2124.856587	5.582490	-0.020712	2.566036
104.461807	2132.942469	5.587494	-0.020752	2.570503
104.943864	2140.979399	5.592499	-0.020847	2.574955
104.893949	2149.053926	5.597504	-0.020843	2.579383
105.209211	2157.106409	5.602509	-0.020907	2.583816
105.323836	2165.165813	5.607514	-0.020934	2.588232
105.630209	2173.351533	5.612518	-0.020996	2.592722
105.869063	2181.423072	5.617523	-0.021046	2.597138
105.935982	2189.422297	5.622528	-0.021064	2.601495
106.369584	2197.406815	5.627533	-0.021150	2.605862
106.688010	2205.408670	5.632538	-0.021214	2.610223
106.868287	2213.488890	5.637542	-0.021253	2.614610
107.116386	2221.503273	5.642547	-0.021304	2.618958
107.474775	2229.524709	5.647552	-0.021376	2.623310
107.845733	2237.564513	5.652557	-0.021451	2.627666
108.120839	2245.628564	5.657562	-0.021507	2.632021
108.512490	2253.686536	5.662566	-0.021586	2.636373
108.671083	2261.732542	5.667571	-0.021620	2.640697
108.860214	2269.766187	5.672576	-0.021661	2.645008
109.353617	2277.804088	5.677581	-0.021758	2.649335
109.702260	2285.868479	5.682586	-0.021828	2.653659
110.106091	2293.902816	5.687590	-0.021909	2.657963
110.403668	2301.955759	5.692595	-0.021969	2.662264
110.606460	2310.012273	5.697600	-0.022012	2.666553
110.797307	2318.103977	5.702605	-0.022053	2.670854
110.751920	2326.202119	5.707610	-0.022050	2.675135
111.234410	2334.191788	5.712614	-0.022145	2.679386
111.668826	2342.198481	5.717619	-0.022231	2.683637
111.862751	2350.234162	5.722624	-0.022273	2.687880
112.288554	2358.321230	5.727629	-0.022357	2.692158
112.355702	2366.378341	5.732634	-0.022375	2.696392
112.398190	2374.437416	5.737638	-0.022388	2.700618
112.825650	2382.447956	5.742643	-0.022473	2.704836
112.948276	2390.492876	5.747648	-0.022501	2.709046
113.241345	2398.568912	5.752653	-0.022561	2.713277
113.614590	2406.589946	5.757658	-0.022636	2.717477
113.724614	2414.657443	5.762662	-0.022662	2.721679
114.015410	2422.697876	5.767667	-0.022721	2.725871
113.924202	2430.758949	5.772672	-0.022709	2.730044
114.374670	2438.812632	5.777677	-0.022798	2.734240
114.702612	2446.823954	5.782682	-0.022865	2.738400
114.788580	2454.889629	5.787686	-0.022886	2.742567
115.191039	2462.905955	5.792691	-0.022966	2.746721
115.539434	2470.972013	5.797696	-0.023036	2.750891
115.831551	2479.114330	5.802701	-0.023096	2.755091
115.927379	2487.105911	5.807706	-0.023119	2.759195
116.221202	2495.116098	5.812710	-0.023179	2.763315
116.591756	2503.157524	5.817715	-0.023253	2.767449
116.715486	2511.208871	5.822720	-0.023282	2.771567
116.929058	2519.284449	5.827725	-0.023327	2.775696
117.253497	2527.289889	5.832730	-0.023392	2.779790
117.487216	2535.320347	5.837734	-0.023441	2.783886
117.558787	2543.408708	5.842739	-0.023460	2.787995
117.777769	2551.424123	5.847744	-0.023506	2.792070
118.111582	2559.498580	5.852749	-0.023573	2.796175
118.224812	2567.511065	5.857754	-0.023600	2.800230
118.610285	2575.518656	5.862758	-0.023677	2.804293
118.814678	2583.555859	5.867763	-0.023720	2.808354
119.200973	2591.590713	5.872768	-0.023797	2.812419
120.010512	2599.615528	5.877773	-0.023953	2.816497
120.489697	2607.615584	5.882778	-0.024048	2.820537
120.700535	2615.667469	5.887782	-0.024092	2.824582
120.854190	2623.761919	5.892787	-0.024126	2.828640
121.230416	2631.810784	5.897792	-0.024202	2.832681
121.817859	2639.850430	5.902797	-0.024316	2.836724
121.840860	2647.889535	5.907802	-0.024326	2.840729
122.190977	2655.901611	5.912806	-0.024396	2.844733
122.373437	2663.969972	5.917811	-0.024435	2.848750
122.598802	2672.036785	5.922816	-0.024483	2.852763
122.721521	2680.096400	5.927821	-0.024511	2.856761
122.916087	2688.130218	5.932826	-0.024552	2.860745
123.398959	2696.113796	5.937830	-0.024647	2.864714
123.483229	2704.200387	5.942835	-0.024668	2.868707
123.761710	2712.237814	5.947840	-0.024726	2.872680
124.194610	2720.280675	5.952845	-0.024811	2.876659
124.218618	2728.323997	5.957850	-0.024821	2.880610
124.328624	2736.348403	5.962854	-0.024847	2.884552
124.866397	2744.361083	5.967859	-0.024952	2.888505
124.901368	2752.438391	5.972864	-0.024964	2.892457
125.260269	2760.485702	5.977869	-0.025036	2.896407
125.564670	2768.493868	5.982874	-0.025098	2.900329
125.537904	2776.567635	5.987878	-0.025098	2.904260
125.868530	2784.605809	5.992883	-0.025165	2.908187
125.948912	2792.714131	5.997888	-0.025186	2.912130
126.343766	2800.773779	6.002893	-0.025264	2.916061
126.334423	2808.765087	6.007898	-0.025268	2.919931
126.559692	2816.761945	6.012902	-0.025315	2.923812
126.921687	2824.778518	6.017907	-0.025388	2.927704
127.112074	2832.824060	6.022912	-0.025428	2.931596
127.253583	2840.885733	6.027917	-0.025460	2.935488
127.419382	2848.889972	6.032922	-0.025496	2.939348
127.830773	2856.895696	6.037926	-0.025578	2.943217
128.129105	2864.949831	6.042931	-0.025639	2.947098
128.313867	2873.008142	6.047936	-0.025679	2.950970
128.524523	2881.078260	6.052941	-0.025723	2.954844
128.646984	2889.110439	6.057946	-0.025751	2.958690
128.755372	2897.140261	6.062950	-0.025777	2.962529
129.178543	2905.144764	6.067955	-0.025861	2.966367
129.274324	2913.198927	6.072960	-0.025884	2.970207
129.570319	2921.265780	6.077965	-0.025944	2.974058
129.566138	2929.312852	6.082970	-0.025949	2.977880
129.847279	2937.331261	6.087974	-0.026006	2.981698
130.080445	2945.358616	6.092979	-0.026055	2.985512
130.131181	2953.385388	6.097984	-0.026070	2.989312
130.638702	2961.437405	6.102989	-0.026169	2.993142
130.903431	2969.458865	6.107994	-0.026224	2.996941
131.008073	2977.514866	6.112998	-0.026249	3.000743
131.306466	2985.495657	6.118003	-0.026310	3.004514
131.615209	2993.513458	6.123008	-0.026372	3.008299
131.798351	3001.603968	6.128013	-0.026412	3.012106
131.780299	3009.669306	6.133018	-0.026414	3.015887
132.239384	3017.660095	6.138022	-0.026504	3.019652
132.460579	3025.683304	6.143027	-0.026551	3.023416
132.910323	3033.696793	6.148032	-0.026640	3.027181
133.025354	3041.774784	6.153037	-0.026667	3.030956
133.298087	3049.815007	6.158042	-0.026723	3.034716
133.616126	3057.845211	6.163046	-0.026787	3.038468
133.733290	3065.890191	6.168051	-0.026814	3.042213
133.949147	3073.918800	6.173056	-0.026860	3.045951
134.162363	3081.965072	6.178061	-0.026905	3.049692
134.348567	3090.007936	6.183066	-0.026945	3.053426
134.694252	3098.017336	6.188070	-0.027014	3.057147
134.690298	3106.089461	6.193075	-0.027019	3.060876
134.882936	3114.082921	6.198080	-0.027060	3.064573
135.145923	3122.134534	6.203085	-0.027114	3.068296
135.462728	3130.202794	6.208090	-0.027178	3.072025
135.482007	3138.317439	6.213094	-0.027187	3.075756
135.817220	3146.272419	6.218099	-0.027255	3.079424
136.076755	3154.269941	6.223104	-0.027308	3.083104
136.359554	3162.297308	6.228109	-0.027366	3.086795
136.398204	3170.341351	6.233114	-0.027379	3.090477
136.587900	3178.385933	6.238118	-0.027419	3.094162
136.860618	3186.407897	6.243123	-0.027475	3.097836
136.972339	3194.432407	6.248128	-0.027502	3.101499
137.179764	3202.452756	6.253133	-0.027545	3.105160
137.358722	3210.492401	6.258138	-0.027584	3.108825
137.482693	3218.549874	6.263142	-0.027612	3.112491
137.893510	3226.595895	6.268147	-0.027694	3.116160
138.032625	3234.578010	6.273152	-0.027725	3.119784
138.245447	3242.613232	6.278157	-0.027770	3.123431
138.430570	3250.654485	6.283162	-0.027810	3.127075
138.724811	3258.690969	6.288166	-0.027870	3.130717
138.980378	3266.751865	6.293171	-0.027923	3.134365
139.279392	3274.753527	6.298176	-0.027984	3.137983
139.624746	3282.786404	6.303181	-0.028053	3.141613
139.950119	3290.805695	6.308186	-0.028119	3.145232
140.066736	3298.849967	6.313190	-0.028146	3.148849
140.544321	3306.903103	6.318195	-0.028240	3.152482
140.760079	3314.937616	6.323200	-0.028286	3.156090
140.865288	3322.966369	6.328205	-0.028311	3.159687
141.009559	3330.964887	6.333210	-0.028343	3.163268
141.241745	3339.006710	6.338214	-0.028391	3.166868
141.669645	3347.037468	6.343219	-0.028476	3.170467
141.828085	3355.078345	6.348224	-0.028511	3.174055
141.968409	3363.145601	6.353229	-0.028542	3.177650
142.186869	3371.156912	6.358234	-0.028588	3.181220
142.483957	3379.143751	6.363238	-0.028649	3.184777
142.664674	3387.223391	6.368243	-0.028688	3.188367
142.819365	3395.254063	6.373248	-0.028722	3.191931
143.085552	3403.326936	6.378253	-0.028777	3.195513
143.074358	3411.323015	6.383258	-0.028780	3.199046
143.488297	3419.285420	6.388262	-0.028862	3.202578
143.590192	3427.377808	6.393267	-0.028887	3.206150
143.855165	3435.359583	6.398272	-0.028941	3.209676
144.175699	3443.433077	6.403277	-0.029006	3.213241
144.430627	3451.462883	6.408282	-0.029059	3.216780
144.591446	3459.479202	6.413286	-0.029094	3.220306
144.697808	3467.511640	6.418291	-0.029119	3.223832
144.946107	3475.545345	6.423296	-0.029171	3.227361
145.071143	3483.613058	6.428301	-0.029199	3.230896
145.028956	3491.728856	6.433306	-0.029197	3.234441
145.209271	3499.699029	6.438310	-0.029235	3.237927
145.480481	3507.691653	6.443315	-0.029291	3.241424
145.561323	3515.698497	6.448320	-0.029311	3.244915
145.678389	3523.737940	6.453325	-0.029339	3.248418
145.897282	3531.760199	6.458330	-0.029385	3.251913
146.245246	3539.795866	6.463334	-0.029455	3.255416
146.466410	3547.798000	6.468339	-0.029501	3.258896
146.468520	3555.844030	6.473344	-0.029507	3.262382
146.714964	3563.910238	6.478349	-0.029558	3.265882
146.736065	3571.904650	6.483354	-0.029567	3.269339
147.038373	3579.964375	6.488358	-0.029629	3.272832
147.421733	3587.992187	6.493363	-0.029705	3.276310
147.534433	3595.976445	6.498368	-0.029731	3.279755
147.647896	3604.027139	6.503373	-0.029758	3.283225
147.961038	3612.060385	6.508378	-0.029821	3.286692
148.021449	3620.085059	6.513382	-0.029838	3.290142
148.127709	3628.154102	6.518387	-0.029863	3.293608
148.382882	3636.144014	6.523392	-0.029916	3.297043
148.918640	3644.148627	6.528397	-0.030021	3.300491
148.759083	3652.205025	6.533402	-0.029996	3.303931
149.075830	3660.200232	6.538406	-0.030061	3.307360
149.284911	3668.278601	6.543411	-0.030105	3.310816
149.569553	3676.318524	6.548416	-0.030163	3.314256
149.866783	3684.332097	6.553421	-0.030224	3.317680
149.975454	3692.333329	6.558426	-0.030249	3.321089
150.235460	3700.327291	6.563430	-0.030303	3.324497
150.287268	3708.395719	6.568435	-0.030318	3.327926
150.465458	3716.434159	6.573440	-0.030356	3.331342
150.643115	3724.486150	6.578445	-0.030395	3.334761
150.735976	3732.494882	6.583450	-0.030417	3.338155
150.859342	3740.530575	6.588454	-0.030445	3.341558
151.111115	3748.541170	6.593459	-0.030498	3.344952
151.144550	3756.563444	6.598464	-0.030509	3.348339
151.360842	3764.632845	6.603469	-0.030555	3.351749
151.633064	3772.665693	6.608474	-0.030611	3.355142
151.749121	3780.663860	6.613478	-0.030637	3.358512
152.071894	3788.703608	6.618483	-0.030703	3.361903
152.270700	3796.693842	6.623488	-0.030745	3.365265
152.543270	3804.735739	6.628493	-0.030801	3.368649
152.727271	3812.794173	6.633498	-0.030841	3.372032
152.913497	3820.823300	6.638502	-0.030881	3.375400
153.294034	3828.811896	6.643507	-0.030957	3.378755
153.500064	3836.826421	6.648512	-0.031000	3.382111
153.626410	3844.882700	6.653517	-0.031029	3.385478
153.891785	3852.910599	6.658522	-0.031084	3.388835
154.272326	3860.976625	6.663526	-0.031160	3.392208
154.445218	3869.072835	6.668531	-0.031197	3.395583
154.467475	3877.010257	6.673536	-0.031207	3.398884
154.595657	3885.043562	6.678541	-0.031236	3.402225
154.776679	3893.039765	6.683546	-0.031275	3.405549
154.963133	3901.037391	6.688550	-0.031315	3.408870
155.398383	3909.097660	6.693555	-0.031401	3.412223
155.407804	3917.131921	6.698560	-0.031408	3.415547
155.576552	3925.143454	6.703565	-0.031445	3.418864
155.803376	3933.148981	6.708570	-0.031492	3.422177
156.152617	3941.156842	6.713574	-0.031563	3.425492
156.236366	3949.212634	6.718579	-0.031583	3.428814
156.216298	3957.270379	6.723584	-0.031585	3.432131
156.708161	3965.312285	6.728589	-0.031682	3.435455
156.820557	3973.289783	6.733594	-0.031708	3.438736
157.109042	3981.313135	6.738598	-0.031767	3.442039
157.397599	3989.338237	6.743603	-0.031826	3.445340
157.500803	3997.363315	6.748608	-0.031850	3.448631
157.450661	4005.458109	6.753613	-0.031846	3.451942
157.649704	4013.470299	6.758618	-0.031889	3.455225
157.931668	4021.466720	6.763622	-0.031946	3.458501
158.145061	4029.518454	6.768627	-0.031991	3.461794
158.293322	4037.514994	6.773632	-0.032024	3.465060
158.480836	4045.565093	6.778637	-0.032064	3.468345
158.580052	4053.640696	6.783642	-0.032088	3.471635
158.625884	4061.665256	6.788646	-0.032102	3.474899
159.088721	4069.646662	6.793651	-0.032193	3.478155
159.220806	4077.668840	6.798656	-0.032223	3.481415
159.347138	4085.658226	6.803661	-0.032252	3.484658
159.544346	4093.708152	6.808666	-0.032294	3.487925
159.837620	4101.721910	6.813670	-0.032354	3.491177
160.349234	4109.730831	6.818675	-0.032454	3.494431
160.282530	4117.763222	6.823680	-0.032447	3.497674
160.615725	4125.808281	6.828685	-0.032515	3.500930
160.820181	4133.789642	6.833690	-0.032558	3.504155
160.838334	4141.847950	6.838694	-0.032567	3.507401
161.387430	4149.851746	6.843699	-0.032674	3.510639
161.416235	4157.928164	6.848704	-0.032685	3.513886
161.628483	4165.951309	6.853709	-0.032730	3.517116
161.702861	4173.948920	6.858714	-0.032749	3.520327
161.798297	4181.959275	6.863718	-0.032772	3.523542
162.220968	4189.994131	6.868723	-0.032856	3.526773
162.349891	4197.991794	6.873728	-0.032885	3.529977
162.468155	4206.089003	6.878733	-0.032912	3.533218
162.838207	4214.127724	6.883738	-0.032986	3.536440
162.733157	4222.112790	6.888742	-0.032972	3.539624
163.074080	4230.165408	6.893747	-0.033041	3.542845
163.017735	4238.205973	6.898752	-0.033036	3.546046
163.307889	4246.223892	6.903757	-0.033095	3.549246
163.461544	4254.307305	6.908762	-0.033129	3.552465
163.790292	4262.350479	6.913766	-0.033195	3.555670
163.942373	4270.337086	6.918771	-0.033229	3.558844
163.805341	4278.323989	6.923776	-0.033209	3.562007
164.203956	4286.338224	6.928781	-0.033288	3.565194
164.290525	4294.352070	6.933786	-0.033309	3.568369
164.464669	4302.382449	6.938790	-0.033347	3.571550
164.677092	4310.441769	6.943795	-0.033392	3.574741
164.890967	4318.415720	6.948800	-0.033437	3.577895
165.207461	4326.475634	6.953805	-0.033501	3.581083
165.296342	4334.431055	6.958810	-0.033523	3.584221
165.554556	4342.469253	6.963814	-0.033576	3.587393
165.825539	4350.515353	6.968819	-0.033632	3.590566
166.124753	4358.530901	6.973824	-0.033693	3.593725
166.278056	4366.580061	6.978829	-0.033727	3.596890
166.600624	4374.554968	6.983834	-0.033792	3.600028
166.618814	4382.557994	6.988838	-0.033801	3.603165
166.920222	4390.609184	6.993843	-0.033862	3.606327
166.980809	4398.594545	6.998848	-0.033879	3.609453
167.220442	4406.697970	7.003853	-0.033929	3.612628
167.504598	4414.723125	7.008858	-0.033987	3.615771
167.783957	4422.689312	7.013862	-0.034044	3.618888
168.044326	4430.721508	7.018867	-0.034098	3.622027
168.051671	4438.724063	7.023872	-0.034104	3.625145
168.111647	4446.775566	7.028877	-0.034121	3.628280
168.560477	4454.829378	7.033882	-0.034210	3.631425
168.729877	4462.852787	7.038886	-0.034246	3.634547
168.850033	4470.918779	7.043891	-0.034274	3.637682
169.238557	4478.889454	7.048896	-0.034352	3.640784
169.424497	4486.895613	7.053901	-0.034392	3.643892
169.510992	4494.934103	7.058906	-0.034413	3.647007
169.537910	4502.943242	7.063910	-0.034423	3.650107
169.802154	4511.017277	7.068915	-0.034478	3.653235
169.740219	4519.038164	7.073920	-0.034471	3.656332
169.939912	4527.052050	7.078925	-0.034514	3.659430
170.131046	4535.052345	7.083930	-0.034555	3.662519
170.199702	4543.105078	7.088934	-0.034573	3.665624
170.531212	4551.152599	7.093939	-0.034640	3.668730
170.638158	4559.137764	7.098944	-0.034665	3.671804
171.071904	4567.189818	7.103949	-0.034751	3.674909
171.115082	4575.190438	7.108954	-0.034764	3.677982
171.276390	4583.224081	7.113958	-0.034800	3.681068
171.497871	4591.206761	7.118963	-0.034846	3.684134
171.537897	4599.228628	7.123968	-0.034859	3.687207
171.653351	4607.271809	7.128973	-0.034886	3.690288
171.853260	4615.302309	7.133978	-0.034928	3.693364
172.100683	4623.294777	7.138982	-0.034979	3.696423
172.353534	4631.330448	7.143987	-0.035032	3.699497
172.742256	4639.308347	7.148992	-0.035109	3.702549
172.798267	4647.381095	7.153997	-0.035125	3.705627
172.850140	4655.393591	7.159002	-0.035140	3.708679
172.803389	4663.455234	7.164006	-0.035136	3.711745
173.197856	4671.546777	7.169011	-0.035215	3.714830
173.441029	4679.492155	7.174016	-0.035266	3.717854
173.517361	4687.507506	7.179021	-0.035285	3.720897
173.790678	4695.504489	7.184026	-0.035341	3.723936
173.910352	4703.517118	7.189030	-0.035369	3.726975
174.033326	4711.560062	7.194035	-0.035397	3.730023
174.113320	4719.580996	7.199040	-0.035417	3.733059
174.411152	4727.628602	7.204045	-0.035478	3.736107
174.411076	4735.591709	7.209050	-0.035483	3.739114
174.643337	4743.619465	7.214054	-0.035532	3.742149
175.050195	4751.647873	7.219059	-0.035613	3.745185
175.036803	4759.669448	7.224064	-0.035615	3.748207
175.056297	4767.748553	7.229069	-0.035624	3.751248
175.388542	4775.750865	7.234074	-0.035691	3.754266
175.563692	4783.789440	7.239078	-0.035729	3.757291
175.844508	4791.788130	7.244083	-0.035787	3.760301
175.832950	4799.802188	7.249088	-0.035790	3.763307
176.017913	4807.866425	7.254093	-0.035830	3.766334
176.342227	4815.840339	7.259098	-0.035895	3.769329
176.373730	4823.894493	7.264102	-0.035906	3.772344
176.604191	4831.916303	7.269107	-0.035955	3.775349
176.652471	4839.911345	7.274112	-0.035969	3.778338
177.024709	4848.002773	7.279117	-0.036044	3.781367
177.174606	4855.958526	7.284122	-0.036077	3.784339
177.533462	4864.018666	7.289126	-0.036149	3.787352
177.526304	4872.077917	7.294131	-0.036153	3.790354
177.733814	4880.081263	7.299136	-0.036197	3.793337
178.008009	4888.100484	7.304141	-0.036253	3.796325
178.171434	4896.057064	7.309146	-0.036289	3.799286
178.198969	4904.088504	7.314150	-0.036299	3.802268
178.703406	4912.059509	7.319155	-0.036398	3.805237
178.423202	4920.128436	7.324160	-0.036351	3.808222
178.453033	4928.166081	7.329165	-0.036362	3.811200
178.868355	4936.190125	7.334170	-0.036445	3.814179
179.092577	4944.171761	7.339174	-0.036492	3.817136
179.366817	4952.200744	7.344179	-0.036548	3.820109
179.333603	4960.192929	7.349184	-0.036547	3.823060
179.644845	4968.234135	7.354189	-0.036610	3.826033
180.004776	4976.234056	7.359194	-0.036682	3.828991
179.968136	4984.307029	7.364198	-0.036681	3.831964
180.334444	4992.341299	7.369203	-0.036754	3.834929
180.539549	5000.354576	7.374208	-0.036798	3.837881
180.642960	5008.354368	7.379213	-0.036822	3.840824
181.013855	5016.320635	7.384218	-0.036897	3.843757
181.348914	5024.368354	7.389222	-0.036964	3.846717
181.550484	5032.395815	7.394227	-0.037007	3.849665
181.593431	5040.469893	7.399232	-0.037020	3.852624
181.904174	5048.473929	7.404237	-0.037084	3.855561
182.169011	5056.513212	7.409242	-0.037138	3.858508
182.081750	5064.513229	7.414246	-0.037127	3.861431
182.381764	5072.502292	7.419251	-0.037188	3.864355
182.601730	5080.577218	7.424256	-0.037234	3.867307
182.703079	5088.616073	7.429261	-0.037259	3.870241
182.867013	5096.835069	7.434266	-0.037294	3.873240
183.098746	5104.830434	7.439270	-0.037343	3.876156
183.330691	5112.753814	7.444275	-0.037391	3.879044
183.471337	5120.725041	7.449280	-0.037423	3.881945
183.662844	5128.701296	7.454285	-0.037464	3.884847
183.868527	5136.743922	7.459290	-0.037507	3.887771
183.997867	5144.727027	7.464294	-0.037536	3.890670
184.099195	5152.764152	7.469299	-0.037561	3.893585
184.163902	5160.818767	7.474304	-0.037578	3.896504
184.359672	5168.781976	7.479309	-0.037620	3.899391
184.370077	5176.838592	7.484314	-0.037627	3.902305
184.363749	5184.813979	7.489318	-0.037631	3.905188
184.832945	5192.861342	7.494323	-0.037724	3.908103
184.852230	5200.865529	7.499328	-0.037732	3.910992
185.218646	5208.914033	7.504333	-0.037806	3.913901
185.290228	5216.965643	7.509338	-0.037824	3.916804
185.402241	5224.906708	7.514342	-0.037851	3.919666
185.713886	5232.959754	7.519347	-0.037914	3.922569
185.842934	5240.943932	7.524352	-0.037943	3.925443
185.903916	5248.988751	7.529357	-0.037960	3.928334
185.913988	5257.031660	7.534362	-0.037967	3.931222
186.113744	5265.016124	7.539366	-0.038009	3.934090
186.609273	5273.073598	7.544371	-0.038107	3.936988
186.471955	5281.056303	7.549376	-0.038087	3.939845
186.495804	5289.066414	7.554381	-0.038096	3.942713
186.963097	5297.111085	7.559386	-0.038189	3.945599
186.987019	5305.119035	7.564390	-0.038198	3.948462
187.114571	5313.197680	7.569395	-0.038227	3.951350
187.212454	5321.204995	7.574400	-0.038251	3.954209
187.545827	5329.195311	7.579405	-0.038318	3.957065
187.585565	5337.190886	7.584410	-0.038331	3.959915
187.729299	5345.167055	7.589414	-0.038363	3.962759
187.993526	5353.230980	7.594419	-0.038417	3.965633
188.214909	5361.223014	7.599424	-0.038464	3.968479
188.491731	5369.299971	7.604429	-0.038520	3.971354
188.760930	5377.324345	7.609434	-0.038576	3.974208
188.824275	5385.322982	7.614438	-0.038593	3.977048
188.875463	5393.366695	7.619443	-0.038608	3.979901
188.938805	5401.358349	7.624448	-0.038625	3.982734
189.276550	5409.368484	7.629453	-0.038693	3.985576
189.399603	5417.441256	7.634458	-0.038721	3.988434
189.638267	5425.450926	7.639462	-0.038771	3.991270
190.037566	5433.509373	7.644467	-0.038850	3.994124
190.055901	5441.508116	7.649472	-0.038859	3.996949
190.019278	5449.490261	7.654477	-0.038857	3.999764
190.210918	5457.533172	7.659482	-0.038898	4.002603
190.257865	5465.512213	7.664486	-0.038912	4.005415
190.452059	5473.566523	7.669491	-0.038954	4.008254
190.827799	5481.582074	7.674496	-0.039029	4.011080
191.009435	5489.642337	7.679501	-0.039068	4.013917
191.032561	5497.649670	7.684506	-0.039078	4.016730
191.286057	5505.624833	7.689510	-0.039130	4.019534
191.488936	5513.667557	7.694515	-0.039173	4.022359
191.599294	5521.662195	7.699520	-0.039199	4.025163
191.938722	5529.719288	7.704525	-0.039267	4.027991
192.290261	5537.762931	7.709530	-0.039338	4.030813
192.450906	5545.866182	7.714534	-0.039373	4.033650
192.394182	5553.898845	7.719539	-0.039368	4.036457
192.482483	5561.795855	7.724544	-0.039390	4.039217
192.936483	5569.813256	7.729549	-0.039480	4.042023
192.950313	5577.797004	7.734554	-0.039487	4.044809
193.262140	5585.813037	7.739558	-0.039551	4.047608
193.553995	5593.865185	7.744563	-0.039610	4.050417
193.420300	5601.897887	7.749568	-0.039591	4.053212
193.686439	5609.921145	7.754573	-0.039645	4.056007
193.924453	5617.869479	7.759578	-0.039695	4.058774
194.060273	5625.917475	7.764582	-0.039726	4.061572
194.313437	5633.931159	7.769587	-0.039778	4.064357
194.288077	5641.947492	7.774592	-0.039779	4.067138
194.510552	5649.971787	7.779597	-0.039825	4.069923
194.680522	5658.034464	7.784602	-0.039862	4.072719
194.792571	5666.013997	7.789606	-0.039888	4.075483
195.150594	5674.012558	7.794611	-0.039960	4.078256
195.205769	5682.062286	7.799616	-0.039976	4.081039
195.465067	5690.019003	7.804621	-0.040029	4.083792
195.497965	5698.086075	7.809626	-0.040041	4.086578
195.674052	5706.058878	7.814630	-0.040079	4.089331
195.797265	5714.127074	7.819635	-0.040107	4.092115
195.889125	5722.171231	7.824640	-0.040129	4.094888
196.067659	5730.182139	7.829645	-0.040168	4.097649
196.266551	5738.204096	7.834650	-0.040210	4.100412
196.250624	5746.178984	7.839654	-0.040212	4.103154
196.497546	5754.231829	7.844659	-0.040264	4.105924
196.855248	5762.225063	7.849664	-0.040335	4.108674
196.834486	5770.286408	7.854669	-0.040337	4.111440
197.086880	5778.366543	7.859674	-0.040389	4.114214
197.524343	5786.318619	7.864678	-0.040476	4.116945
197.651700	5794.314199	7.869683	-0.040505	4.119685
197.673598	5802.328209	7.874688	-0.040514	4.122428
198.026056	5810.292427	7.879693	-0.040585	4.125156
198.243737	5818.383991	7.884698	-0.040631	4.127924
198.046021	5826.425882	7.889702	-0.040599	4.130668
198.270024	5834.481483	7.894707	-0.040646	4.133421
198.483058	5842.448644	7.899712	-0.040691	4.136141
198.635085	5850.461823	7.904717	-0.040725	4.138874
198.986123	5858.551170	7.909722	-0.040795	4.141634
199.231958	5866.454402	7.914726	-0.040846	4.144327
199.299137	5874.570261	7.919731	-0.040864	4.147089
199.497787	5882.567509	7.924736	-0.040906	4.149810
199.762176	5890.585258	7.929741	-0.040961	4.152537
199.950260	5898.607374	7.934746	-0.041001	4.155263
199.936739	5906.605929	7.939750	-0.041004	4.157977
199.976430	5914.644722	7.944755	-0.041016	4.160703
200.225173	5922.604226	7.949760	-0.041068	4.163403
200.376379	5930.653490	7.954765	-0.041101	4.166130
200.677956	5938.679010	7.959770	-0.041163	4.168850
200.837016	5946.692537	7.964774	-0.041198	4.171561
201.062319	5954.721147	7.969779	-0.041245	4.174277
201.081620	5962.765642	7.974784	-0.041254	4.176994
201.367981	5970.740855	7.979789	-0.041312	4.179689
201.616857	5978.759610	7.984794	-0.041364	4.182397
201.648685	5986.750928	7.989798	-0.041375	4.185091
202.029347	5994.815808	7.994803	-0.041451	4.187811
202.151947	6002.793313	7.999808	-0.041479	4.190498
202.126717	6010.948773	8.004813	-0.041480	4.193241
202.642074	6018.939967	8.009818	-0.041581	4.195934
202.622547	6026.850303	8.014822	-0.041583	4.198591
202.931062	6034.888314	8.019827	-0.041645	4.201293
202.925499	6042.858641	8.024832	-0.041650	4.203967
203.142060	6050.914676	8.029837	-0.041695	4.206671
203.352316	6058.900697	8.034842	-0.041740	4.209349
203.466407	6066.940551	8.039846	-0.041766	4.212043
203.713918	6074.967531	8.044851	-0.041818	4.214732
204.044563	6082.940262	8.049856	-0.041884	4.217402
204.152336	6090.969762	8.054861	-0.041910	4.220087
204.149238	6099.003075	8.059866	-0.041914	4.222770
204.283262	6107.002806	8.064870	-0.041945	4.225442
204.499018	6115.026775	8.069875	-0.041990	4.228121
204.446071	6123.065700	8.074880	-0.041985	4.230801
204.878025	6131.087113	8.079885	-0.042071	4.233478
205.014256	6139.144874	8.084890	-0.042102	4.236162
205.108040	6147.114241	8.089894	-0.042124	4.238815
205.358825	6155.163978	8.094899	-0.042176	4.241494
205.387217	6163.092737	8.099904	-0.042187	4.244129
205.494450	6171.156799	8.104909	-0.042212	4.246808
205.762471	6179.199856	8.109914	-0.042267	4.249481
205.798446	6187.203712	8.114918	-0.042279	4.252136
206.205151	6195.253217	8.119923	-0.042360	4.254808
206.052435	6203.237528	8.124928	-0.042337	4.257452
206.382173	6211.259817	8.129933	-0.042404	4.260111
206.588025	6219.317984	8.134938	-0.042447	4.262779
206.343086	6227.311235	8.139942	-0.042407	4.265420
206.597983	6235.365004	8.144947	-0.042460	4.268083
206.552515	6243.381750	8.149952	-0.042456	4.270731
206.805795	6251.414531	8.154957	-0.042509	4.273384
206.987458	6259.467539	8.159962	-0.042548	4.276042
207.316521	6267.349393	8.164966	-0.042614	4.278643
207.665277	6275.443288	8.169971	-0.042685	4.281312
207.610506	6283.400900	8.174976	-0.042680	4.283931
207.699108	6291.473640	8.179981	-0.042702	4.286588
207.964529	6299.454863	8.184986	-0.042756	4.289215
208.363058	6307.542317	8.189990	-0.042836	4.291876
208.234870	6315.562395	8.194995	-0.042817	4.294508
208.396822	6323.546930	8.200000	-0.042852	4.297130
208.658345	6331.533991	8.205005	-0.042906	4.299752
208.797969	6339.580429	8.210010	-0.042938	4.302391
208.802637	6347.561699	8.215014	-0.042944	4.305005
209.105021	6355.640916	8.220019	-0.043005	4.307653
209.191732	6363.632958	8.225024	-0.043027	4.310268
209.407836	6371.669852	8.230029	-0.043072	4.312898
209.502933	6379.698304	8.235034	-0.043095	4.315523
209.692036	6387.650162	8.240038	-0.043136	4.318121
209.925911	6395.691986	8.245043	-0.043184	4.320747
210.103601	6403.708480	8.250048	-0.043223	4.323364
210.218145	6411.719827	8.255053	-0.043249	4.325976
210.346306	6419.725224	8.260058	-0.043279	4.328585
210.312783	6427.757291	8.265062	-0.043278	4.331200
210.914480	6435.822584	8.270067	-0.043395	4.333829
210.985783	6443.852628	8.275072	-0.043413	4.336441
211.062482	6451.800954	8.280077	-0.043433	4.339025
211.302681	6459.869809	8.285082	-0.043483	4.341647
211.402926	6467.819598	8.290086	-0.043507	4.344228
211.566187	6475.864299	8.295091	-0.043542	4.346839
211.699741	6483.901039	8.300096	-0.043573	4.349446
212.028388	6491.924217	8.305101	-0.043639	4.352048
212.120848	6500.040055	8.310106	-0.043662	4.354676
212.308173	6507.983315	8.315110	-0.043702	4.357248
212.371160	6515.949268	8.320115	-0.043719	4.359825
212.401668	6523.988233	8.325120	-0.043730	4.362424
212.412477	6531.906726	8.330125	-0.043737	4.364982
212.718024	6539.995399	8.335130	-0.043799	4.367596
212.761324	6547.979846	8.340134	-0.043812	4.370172
212.831506	6556.015974	8.345139	-0.043831	4.372764
213.171715	6563.999533	8.350144	-0.043899	4.375339
213.539764	6572.015542	8.355149	-0.043973	4.377923
213.490250	6580.065427	8.360154	-0.043969	4.380514
213.516207	6588.049777	8.365158	-0.043979	4.383083
214.059270	6596.078132	8.370163	-0.044086	4.385667
214.116660	6604.116165	8.375168	-0.044101	4.388250
214.073871	6612.115987	8.380173	-0.044099	4.390819
214.270901	6620.175683	8.385178	-0.044141	4.393407
214.515018	6628.173206	8.390182	-0.044191	4.395974
214.576417	6636.196138	8.395187	-0.044208	4.398546
214.477531	6644.190417	8.400192	-0.044195	4.401107
214.694114	6652.157764	8.405197	-0.044240	4.403659
214.730908	6660.242068	8.410202	-0.044253	4.406246
214.951368	6668.216860	8.415206	-0.044299	4.408798
215.217539	6676.298228	8.420211	-0.044354	4.411382
215.593819	6684.297659	8.425216	-0.044429	4.413939
215.567865	6692.345323	8.430221	-0.044430	4.416508
215.952564	6700.319904	8.435226	-0.044506	4.419055
215.816624	6708.354160	8.440230	-0.044486	4.421616
215.838359	6716.362247	8.445235	-0.044496	4.424168
216.022586	6724.419633	8.450240	-0.044535	4.426735
216.398541	6732.384796	8.455245	-0.044610	4.429273
216.638864	6740.478360	8.460250	-0.044661	4.431849
216.503723	6748.456351	8.465254	-0.044641	4.434385
216.886916	6756.494493	8.470259	-0.044717	4.436941
216.927466	6764.448750	8.475264	-0.044730	4.439467
217.201072	6772.531308	8.480269	-0.044786	4.442034
217.164620	6780.509609	8.485274	-0.044785	4.444564
217.367160	6788.529672	8.490278	-0.044828	4.447108
217.504023	6796.504020	8.495283	-0.044858	4.449635
217.598727	6804.599873	8.500288	-0.044881	4.452199
217.819978	6812.573522	8.505293	-0.044928	4.454724
218.003139	6820.650993	8.510298	-0.044967	4.457279
217.858311	6828.590012	8.515302	-0.044945	4.459788
218.093990	6836.655377	8.520307	-0.044995	4.462338
218.169084	6844.635386	8.525312	-0.045014	4.464858
218.460253	6852.625331	8.530317	-0.045073	4.467380
218.593630	6860.660344	8.535322	-0.045103	4.469915
218.730132	6868.693008	8.540326	-0.045134	4.472447
218.837908	6876.736554	8.545331	-0.045159	4.474982
218.893472	6884.742630	8.550336	-0.045175	4.477503
219.136590	6892.703606	8.555341	-0.045225	4.480009
219.633654	6900.723069	8.560346	-0.045323	4.482533
219.648879	6908.704541	8.565351	-0.045331	4.485042
219.744337	6916.787102	8.570355	-0.045354	4.487581
219.918709	6924.785975	8.575360	-0.045392	4.490093
220.130943	6932.820882	8.580365	-0.045437	4.492615
220.036205	6940.872286	8.585370	-0.045424	4.495140
220.281873	6948.838325	8.590375	-0.045475	4.497637
220.441887	6956.867500	8.595379	-0.045511	4.500153
220.753994	6964.885911	8.600384	-0.045574	4.502664
220.902719	6972.839503	8.605389	-0.045607	4.505154
221.222313	6980.941887	8.610394	-0.045672	4.507688
221.171850	6988.896199	8.615399	-0.045667	4.510174
221.344018	6997.001021	8.620403	-0.045705	4.512707
221.413995	7005.013262	8.625408	-0.045723	4.515208
221.496732	7012.972836	8.630413	-0.045744	4.517692
221.670151	7021.019255	8.635418	-0.045781	4.520202
221.681462	7028.974236	8.640423	-0.045789	4.522681
221.904897	7036.997226	8.645427	-0.045835	4.525181
221.998514	7045.014624	8.650432	-0.045858	4.527678
222.376237	7053.013480	8.655437	-0.045934	4.530167
222.520537	7061.078687	8.660442	-0.045966	4.532676
222.635170	7069.109434	8.665447	-0.045992	4.535172
222.732052	7077.129691	8.670451	-0.046016	4.537664
223.072833	7085.121747	8.675456	-0.046084	4.540146
223.043626	7093.088277	8.680461	-0.046084	4.542618
223.250273	7101.110170	8.685466	-0.046128	4.545106
223.495479	7109.118202	8.690471	-0.046179	4.547589
223.677744	7117.145158	8.695475	-0.046218	4.550076
223.762159	7125.216417	8.700480	-0.046239	4.552575
223.796053	7133.245976	8.705485	-0.046251	4.555060
224.116832	7141.264464	8.710490	-0.046316	4.557540
224.194513	7149.223885	8.715495	-0.046335	4.560001
224.307333	7157.256228	8.720499	-0.046362	4.562482
224.425120	7165.209032	8.725504	-0.046389	4.564938
224.683559	7173.231399	8.730509	-0.046442	4.567414
224.780665	7181.269962	8.735514	-0.046466	4.569894
224.835953	7189.317137	8.740519	-0.046481	4.572374
225.081232	7197.356932	8.745523	-0.046532	4.574852
225.076334	7205.414138	8.750528	-0.046536	4.577333
225.232772	7213.379870	8.755533	-0.046571	4.579784
225.485054	7221.424805	8.760538	-0.046623	4.582259
225.669799	7229.371771	8.765543	-0.046663	4.584703
225.920363	7237.390997	8.770547	-0.046715	4.587167
226.201992	7245.464403	8.775552	-0.046772	4.589646
226.228928	7253.490898	8.780557	-0.046783	4.592110
226.214383	7261.557425	8.785562	-0.046785	4.594584
226.500286	7269.524961	8.790567	-0.046844	4.597027
226.647330	7277.495006	8.795571	-0.046876	4.599470
226.782775	7285.537681	8.800576	-0.046907	4.601933
226.801094	7293.473639	8.805581	-0.046915	4.604362
227.042689	7301.577967	8.810586	-0.046966	4.606842
226.946638	7309.525599	8.815591	-0.046953	4.609272
227.324359	7317.599828	8.820595	-0.047029	4.611739
227.410858	7325.599871	8.825600	-0.047050	4.614183
227.452608	7333.682962	8.830605	-0.047063	4.616651
227.560197	7341.652715	8.835610	-0.047088	4.619082
227.733636	7349.686135	8.840615	-0.047126	4.621532
227.837548	7357.643937	8.845619	-0.047150	4.623958
227.767963	7365.679639	8.850624	-0.047143	4.626406
227.882831	7373.680781	8.855629	-0.047169	4.628842
228.297212	7381.737849	8.860634	-0.047252	4.631293
228.369348	7389.761928	8.865639	-0.047270	4.633734
228.508942	7397.794487	8.870643	-0.047302	4.636176
228.573778	7405.756180	8.875648	-0.047319	4.638595
228.629391	7413.763179	8.880653	-0.047335	4.641026
228.788164	7421.772569	8.885658	-0.047369	4.643457
228.869263	7429.780897	8.890663	-0.047390	4.645886
229.156658	7437.793976	8.895667	-0.047449	4.648315
229.444693	7445.848468	8.900672	-0.047507	4.650756
229.291166	7453.840033	8.905677	-0.047484	4.653176
229.541495	7461.933937	8.910682	-0.047536	4.655626
229.793261	7469.909385	8.915687	-0.047588	4.658039
229.890302	7477.868910	8.920691	-0.047611	4.660445
230.151836	7485.912763	8.925696	-0.047665	4.662876
230.181061	7493.899024	8.930701	-0.047676	4.665289
230.331839	7501.969580	8.935706	-0.047709	4.667725
230.567099	7509.952675	8.940711	-0.047758	4.670134
230.871509	7518.029346	8.945715	-0.047820	4.672569
230.991672	7526.097066	8.950720	-0.047848	4.675001
230.790732	7534.042060	8.955725	-0.047816	4.677395
230.927122	7541.972020	8.960730	-0.047847	4.679783
231.074087	7550.031693	8.965735	-0.047879	4.682208
231.106483	7558.032699	8.970739	-0.047890	4.684615
231.226749	7566.063263	8.975744	-0.047918	4.687029
231.520061	7573.995111	8.980749	-0.047978	4.689412
231.681244	7582.101874	8.985754	-0.048013	4.691847
231.647354	7590.081670	8.990759	-0.048012	4.694242
231.926664	7598.166424	8.995763	-0.048069	4.696667
232.163281	7606.113565	9.000768	-0.048119	4.699050
232.318428	7614.148678	9.005773	-0.048153	4.701458
232.431070	7622.134516	9.010778	-0.048179	4.703850
232.710664	7630.183036	9.015783	-0.048236	4.706259
232.779253	7638.172669	9.020787	-0.048254	4.708650
233.127179	7646.234291	9.025792	-0.048325	4.711061
232.910478	7654.273853	9.030797	-0.048289	4.713465
233.093142	7662.298683	9.035802	-0.048329	4.715862
233.244096	7670.221805	9.040807	-0.048362	4.718228
233.482906	7678.245952	9.045811	-0.048412	4.720622
233.437035	7686.265557	9.050816	-0.048408	4.723015
233.484683	7694.295273	9.055821	-0.048423	4.725409
233.688829	7702.357731	9.060826	-0.048466	4.727812
233.915804	7710.350155	9.065831	-0.048513	4.730192
233.985419	7718.406063	9.070835	-0.048532	4.732590
234.007659	7726.419468	9.075840	-0.048541	4.734975
234.276003	7734.396277	9.080845	-0.048596	4.737347
234.575154	7742.411114	9.085850	-0.048657	4.739728
234.435201	7750.386776	9.090855	-0.048636	4.742099
234.538999	7758.399390	9.095859	-0.048661	4.744478
234.982752	7766.448050	9.100864	-0.048749	4.746866
235.164334	7774.452876	9.105869	-0.048788	4.749240
235.293637	7782.506499	9.110874	-0.048817	4.751628
235.512060	7790.584185	9.115879	-0.048863	4.754021
235.662098	7798.581981	9.120883	-0.048896	4.756390
235.639184	7806.539655	9.125888	-0.048897	4.758746
235.983352	7814.544601	9.130893	-0.048967	4.761113
235.967053	7822.520888	9.135898	-0.048969	4.763473
235.981061	7830.565930	9.140903	-0.048977	4.765851
236.419677	7838.525095	9.145907	-0.049064	4.768201
236.614404	7846.629126	9.150912	-0.049105	4.770594
236.605276	7854.615188	9.155917	-0.049109	4.772951
236.771776	7862.677314	9.160922	-0.049145	4.775330
236.901291	7870.640330	9.165927	-0.049174	4.777677
236.961798	7878.626537	9.170931	-0.049191	4.780031
236.894245	7886.717812	9.175936	-0.049184	4.782415
237.430366	7894.611344	9.180941	-0.049289	4.784737
237.610323	7902.758657	9.185946	-0.049327	4.787134
237.371547	7910.630372	9.190951	-0.049288	4.789451
237.514058	7918.765074	9.195955	-0.049320	4.791842
237.759083	7926.779987	9.200960	-0.049371	4.794196
237.943089	7934.818251	9.205965	-0.049410	4.796556
237.813718	7942.749548	9.210970	-0.049392	4.798885
238.048122	7950.767795	9.215975	-0.049440	4.801237
238.469224	7958.775869	9.220979	-0.049524	4.803584
238.365161	7966.849197	9.225984	-0.049510	4.805951
238.306861	7974.797159	9.230989	-0.049504	4.808280
238.637415	7982.874516	9.235994	-0.049571	4.810644
238.780926	7990.408911	9.240999	-0.049603	4.812849
238.950154	7995.116969	9.246003	-0.049638	4.814226

238.927636	7997.721673	9.251008	-0.049635	4.814988
239.105238	7998.966924	9.256013	-0.049669	4.815351
239.194341	7999.411337	9.261018	-0.049686	4.815481
239.357211	8000.524123	9.266023	-0.049717	4.815805
239.354394	8000.568915	9.271027	-0.049717	4.815818
239.287417	8000.524066	9.276032	-0.049704	4.815806
239.380723	8000.530918	9.281037	-0.049721	4.815807
239.655747	8000.566332	9.286042	-0.049773	4.815816
239.397854	8000.493838	9.291047	-0.049725	4.815796
239.312686	8000.534094	9.296051	-0.049709	4.815808
239.644076	8000.452997	9.301056	-0.049771	4.815783
239.774194	8000.541574	9.306061	-0.049795	4.815808
239.566821	8000.571311	9.311066	-0.049756	4.815818
239.528582	8000.549344	9.316071	-0.049749	4.815812
239.486174	8000.550795	9.321075	-0.049741	4.815813
239.656387	8000.561027	9.326080	-0.049773	4.815815
239.663783	8000.517382	9.331085	-0.049774	4.815802
240.048372	8000.543897	9.336090	-0.049846	4.815808
239.787976	8000.512994	9.341095	-0.049798	4.815800
239.959436	8000.563812	9.346099	-0.049830	4.815814
240.238777	8000.443442	9.351104	-0.049882	4.815778
239.984332	8000.553546	9.356109	-0.049834	4.815811
239.928916	8000.559056	9.361114	-0.049824	4.815813
239.993701	8000.540893	9.366119	-0.049836	4.815807
240.002127	8000.569855	9.371123	-0.049838	4.815816
239.826665	8000.546733	9.376128	-0.049805	4.815810
239.901772	8000.536210	9.381133	-0.049819	4.815806
239.999705	8000.561284	9.386138	-0.049837	4.815813
239.988010	8000.530140	9.391143	-0.049835	4.815804
239.920446	8000.481011	9.396147	-0.049823	4.815790
240.005157	8000.570988	9.401152	-0.049839	4.815816
240.168150	8000.465814	9.406157	-0.049869	4.815784
240.198562	8000.560250	9.411162	-0.049875	4.815812
240.083080	8000.548774	9.416167	-0.049853	4.815809
240.389184	8000.588964	9.421171	-0.049910	4.815819
240.445066	8000.479918	9.426176	-0.049921	4.815787
240.323278	8000.570822	9.431181	-0.049898	4.815814
240.407670	8000.572192	9.436186	-0.049914	4.815814
240.371718	8000.555599	9.441191	-0.049907	4.815810
240.282657	8000.570172	9.446195	-0.049890	4.815814
240.572496	8000.556723	9.451200	-0.049944	4.815809
240.316808	8000.513085	9.456205	-0.049897	4.815798
240.122234	8000.538758	9.461210	-0.049861	4.815806
240.118519	8000.533363	9.466215	-0.049860	4.815804
240.272733	8000.541202	9.471219	-0.049889	4.815806
240.355516	8000.471023	9.476224	-0.049904	4.815785
240.248144	8000.545079	9.481229	-0.049884	4.815807
240.332290	8000.587011	9.486234	-0.049900	4.815819
240.473997	8000.545541	9.491239	-0.049926	4.815806
240.368274	8000.470173	9.496243	-0.049907	4.815785
240.547331	8000.565951	9.501248	-0.049940	4.815812
240.631439	8000.521413	9.506253	-0.049956	4.815798
240.745145	8000.575567	9.511258	-0.049977	4.815814
240.633765	8000.559887	9.516263	-0.049956	4.815810
240.674247	8000.554141	9.521267	-0.049964	4.815808
240.694633	8000.474410	9.526272	-0.049968	4.815784
240.432078	8000.536344	9.531277	-0.049919	4.815804
240.641355	8000.576034	9.536282	-0.049958	4.815814
240.540928	8000.566937	9.541287	-0.049939	4.815812
240.440363	8000.470301	9.546291	-0.049920	4.815784
240.533236	8000.571088	9.551296	-0.049938	4.815813
240.457505	8000.571998	9.556301	-0.049924	4.815814
240.518653	8000.507873	9.561306	-0.049935	4.815795
240.413227	8000.564881	9.566311	-0.049916	4.815812
240.553801	8000.577837	9.571315	-0.049942	4.815815
240.664958	8000.492104	9.576320	-0.049962	4.815790
240.678698	8000.559584	9.581325	-0.049965	4.815809
240.776626	8000.570781	9.586330	-0.049983	4.815812
240.801727	8000.483654	9.591335	-0.049988	4.815787
240.800942	8000.516737	9.596339	-0.049988	4.815796
241.016997	8000.581090	9.601344	-0.050028	4.815814
240.933204	8000.467644	9.606349	-0.050013	4.815781
241.002867	8000.583002	9.611354	-0.050026	4.815815
240.761812	8000.557747	9.616359	-0.049981	4.815808
240.749890	8000.576772	9.621363	-0.049979	4.815814
240.795443	8000.492111	9.626368	-0.049987	4.815789
240.758488	8000.582255	9.631373	-0.049980	4.815816
240.859482	8000.593502	9.636378	-0.049999	4.815818
240.855321	8000.543264	9.641383	-0.049998	4.815804
240.876370	8000.588444	9.646387	-0.050002	4.815817
240.877699	8000.526551	9.651392	-0.050003	4.815799
240.815478	8000.492453	9.656397	-0.049991	4.815789
241.076539	8000.594899	9.661402	-0.050040	4.815818
241.054512	8000.484589	9.666407	-0.050036	4.815786
240.828180	8000.586609	9.671411	-0.049993	4.815817
240.976035	8000.472647	9.676416	-0.050021	4.815783
240.815618	8000.559723	9.681421	-0.049991	4.815809
240.932640	8000.527461	9.686426	-0.050013	4.815799
240.803278	8000.514692	9.691431	-0.049989	4.815796
240.979528	8000.581603	9.696435	-0.050022	4.815814
241.006182	8000.582038	9.701440	-0.050027	4.815814
240.933442	8000.544566	9.706445	-0.050013	4.815804
241.182784	8000.566758	9.711450	-0.050060	4.815809
240.761383	8000.533243	9.716455	-0.049981	4.815801
240.921480	8000.484599	9.721459	-0.050011	4.815786
240.950481	8000.570474	9.726464	-0.050017	4.815811
241.129740	8000.548828	9.731469	-0.050050	4.815804
241.070962	8000.563892	9.736474	-0.050039	4.815809
241.032589	8000.565408	9.741479	-0.050032	4.815809
240.990192	8000.556183	9.746483	-0.050024	4.815807
241.081856	8000.560874	9.751488	-0.050041	4.815808
241.147570	8000.546996	9.756493	-0.050053	4.815803
241.110057	8000.586957	9.761498	-0.050047	4.815815
241.223621	8000.554640	9.766503	-0.050068	4.815805
241.213839	8000.575835	9.771507	-0.050066	4.815812
241.450483	8000.483595	9.776512	-0.050110	4.815784
241.037304	8000.548426	9.781517	-0.050033	4.815804
241.124874	8000.570131	9.786522	-0.050049	4.815810
241.007000	8000.560750	9.791527	-0.050028	4.815808
241.066300	8000.493392	9.796531	-0.050039	4.815788
241.075515	8000.581082	9.801536	-0.050040	4.815814
241.257195	8000.578692	9.806541	-0.050074	4.815812
241.110766	8000.494121	9.811546	-0.050047	4.815788
241.076771	8000.546950	9.816551	-0.050041	4.815804
241.169243	8000.552721	9.821555	-0.050058	4.815805
241.348367	8000.569505	9.826560	-0.050091	4.815809
241.101141	8000.570839	9.831565	-0.050045	4.815811
241.107826	8000.490885	9.836570	-0.050047	4.815787
241.130633	8000.572390	9.841575	-0.050051	4.815811
241.158309	8000.572841	9.846579	-0.050056	4.815811
241.279471	8000.578010	9.851584	-0.050079	4.815812
241.306214	8000.470625	9.856589	-0.050084	4.815780
241.322263	8000.581912	9.861594	-0.050087	4.815813
241.256948	8000.489048	9.866599	-0.050074	4.815786
241.080398	8000.604686	9.871603	-0.050042	4.815821
241.320552	8000.490084	9.876608	-0.050086	4.815786
241.244347	8000.566782	9.881613	-0.050072	4.815809
241.163291	8000.584687	9.886618	-0.050057	4.815814
241.316749	8000.561556	9.891623	-0.050086	4.815807
241.301994	8000.574130	9.896627	-0.050083	4.815811
241.094160	8000.570764	9.901632	-0.050044	4.815811
241.023194	8000.468202	9.906637	-0.050031	4.815781
241.171391	8000.600845	9.911642	-0.050059	4.815819
241.333891	8000.554375	9.916647	-0.050089	4.815805
241.328158	8000.474220	9.921651	-0.050088	4.815781
241.368937	8000.570962	9.926656	-0.050096	4.815809
241.290014	8000.570753	9.931661	-0.050081	4.815810
241.324105	8000.594794	9.936666	-0.050088	4.815817
241.349164	8000.519408	9.941671	-0.050092	4.815794
241.202927	8000.537324	9.946675	-0.050065	4.815800
241.294977	8000.588993	9.951680	-0.050082	4.815815
241.157249	8000.570750	9.956685	-0.050057	4.815810
241.171550	8000.485582	9.961690	-0.050059	4.815785
241.211613	8000.539610	9.966695	-0.050067	4.815801
241.233770	8000.575201	9.971699	-0.050071	4.815811
241.299338	8000.565591	9.976704	-0.050083	4.815808
241.160697	8000.538794	9.981709	-0.050057	4.815801
241.250744	8000.578687	9.986714	-0.050074	4.815812
241.267956	8000.477553	9.991719	-0.050077	4.815783
241.328787	8000.578890	9.996723	-0.050089	4.815812
241.321314	8000.561691	10.001728	-0.050087	4.815807
241.306566	8000.564658	10.006733	-0.050085	4.815808
241.533889	8000.583291	10.011738	-0.050127	4.815812
241.355302	8000.562250	10.016743	-0.050094	4.815807
241.241612	8000.570018	10.021747	-0.050073	4.815810
241.501683	8000.386350	10.026752	-0.050121	4.815755
241.459980	8000.583171	10.031757	-0.050113	4.815813
241.428672	8000.497263	10.036762	-0.050108	4.815788
241.316502	8000.579784	10.041767	-0.050087	4.815812
241.443696	8000.582916	10.046771	-0.050110	4.815813
241.318277	8000.476267	10.051776	-0.050087	4.815782
241.330618	8000.591764	10.056781	-0.050089	4.815816
241.286757	8000.581448	10.061786	-0.050081	4.815813
241.211064	8000.549265	10.066791	-0.050067	4.815804
241.103060	8000.579543	10.071795	-0.050047	4.815813
241.361357	8000.490857	10.076800	-0.050095	4.815786
241.369667	8000.567857	10.081805	-0.050097	4.815808
241.393967	8000.597077	10.086810	-0.050101	4.815817
241.313719	8000.474080	10.091815	-0.050086	4.815781
241.401877	8000.574793	10.096819	-0.050103	4.815810
241.402925	8000.510760	10.101824	-0.050103	4.815792
241.243661	8000.590382	10.106829	-0.050074	4.815816
241.431228	8000.582750	10.111834	-0.050109	4.815813
241.450782	8000.478450	10.116839	-0.050112	4.815782
241.397881	8000.588620	10.121843	-0.050102	4.815814
241.341409	8000.484156	10.126848	-0.050092	4.815784
241.219067	8000.561174	10.131853	-0.050069	4.815807
241.411391	8000.579239	10.136858	-0.050105	4.815812
241.223003	8000.574053	10.141863	-0.050070	4.815811
241.457630	8000.586400	10.146867	-0.050114	4.815813
241.366114	8000.494178	10.151872	-0.050097	4.815787
241.308329	8000.577580	10.156877	-0.050086	4.815812
241.437210	8000.510282	10.161882	-0.050110	4.815791
241.687964	8000.496201	10.166887	-0.050157	4.815786
241.542954	8000.597405	10.171891	-0.050130	4.815816
241.596161	8000.586527	10.176896	-0.050140	4.815813
241.403996	8000.500146	10.181901	-0.050104	4.815789
241.334669	8000.497958	10.186906	-0.050091	4.815788
241.345501	8000.580337	10.191911	-0.050093	4.815812
241.568965	8000.496423	10.196915	-0.050135	4.815787
241.515236	8000.580959	10.201920	-0.050125	4.815812
241.360788	8000.497325	10.206925	-0.050096	4.815788
241.469914	8000.595175	10.211930	-0.050116	4.815816
241.447629	8000.580939	10.216935	-0.050112	4.815812
241.359421	8000.501581	10.221939	-0.050096	4.815789
241.313335	8000.595848	10.226944	-0.050087	4.815817
241.285623	8000.575118	10.231949	-0.050082	4.815811
241.456962	8000.510643	10.236954	-0.050114	4.815791
241.564292	8000.485697	10.241959	-0.050134	4.815784
241.606130	8000.579255	10.246963	-0.050142	4.815811
241.527102	8000.579044	10.251968	-0.050127	4.815811
241.453183	8000.481770	10.256973	-0.050114	4.815783
241.435363	8000.598913	10.261978	-0.050110	4.815817
241.565760	8000.562598	10.266983	-0.050135	4.815806
241.579949	8000.591655	10.271987	-0.050137	4.815814
241.430725	8000.489957	10.276992	-0.050109	4.815785
241.497715	8000.552963	10.281997	-0.050122	4.815803
241.457512	8000.583273	10.287002	-0.050115	4.815813
241.380131	8000.569211	10.292007	-0.050100	4.815809
241.520199	8000.569349	10.297011	-0.050126	4.815808
241.722488	8000.487227	10.302016	-0.050164	4.815783
241.530713	8000.581268	10.307021	-0.050128	4.815812
241.536328	8000.582429	10.312026	-0.050129	4.815812
241.726042	8000.559887	10.317031	-0.050165	4.815804
241.618988	8000.580572	10.322035	-0.050145	4.815811
241.549215	8000.488703	10.327040	-0.050132	4.815784
241.500693	8000.567985	10.332045	-0.050123	4.815808
241.603067	8000.588863	10.337050	-0.050142	4.815813
241.481436	8000.560205	10.342055	-0.050119	4.815806
241.484020	8000.589074	10.347059	-0.050120	4.815814
241.754899	8000.401309	10.352064	-0.050170	4.815758
241.527942	8000.576981	10.357069	-0.050128	4.815810
241.664975	8000.501274	10.362074	-0.050154	4.815788
241.619199	8000.566723	10.367079	-0.050145	4.815807
241.632295	8000.571208	10.372083	-0.050148	4.815808
241.527887	8000.591937	10.377088	-0.050128	4.815815
241.586819	8000.569409	10.382093	-0.050139	4.815808
241.744371	8000.506845	10.387098	-0.050169	4.815789
241.730544	8000.576014	10.392103	-0.050166	4.815809
241.751383	8000.591301	10.397107	-0.050170	4.815813
241.869517	8000.503544	10.402112	-0.050192	4.815787
241.618230	8000.587013	10.407117	-0.050145	4.815813
241.627179	8000.488946	10.412122	-0.050147	4.815784
241.769096	8000.574518	10.417127	-0.050173	4.815808
241.848350	8000.509618	10.422131	-0.050188	4.815789
241.638166	8000.533969	10.427136	-0.050149	4.815797
241.478460	8000.537789	10.432141	-0.050119	4.815799
241.652304	8000.603595	10.437146	-0.050152	4.815818
241.577868	8000.578905	10.442151	-0.050138	4.815811
241.519049	8000.501091	10.447155	-0.050127	4.815788
241.444228	8000.504151	10.452160	-0.050113	4.815789
241.559084	8000.589284	10.457165	-0.050135	4.815814
241.572842	8000.487026	10.462170	-0.050137	4.815784
241.640008	8000.499860	10.467175	-0.050150	4.815787
241.496746	8000.588282	10.472179	-0.050123	4.815814
241.604254	8000.482205	10.477184	-0.050143	4.815782
241.810246	8000.577357	10.482189	-0.050182	4.815809
241.729941	8000.500261	10.487194	-0.050167	4.815787
241.823829	8000.558366	10.492199	-0.050184	4.815803
241.742893	8000.564530	10.497203	-0.050169	4.815806
241.981647	8000.497945	10.502208	-0.050213	4.815785
241.783668	8000.568399	10.507213	-0.050177	4.815807
241.727297	8000.584569	10.512218	-0.050166	4.815812
241.779497	8000.569405	10.517223	-0.050176	4.815807
241.925018	8000.576037	10.522227	-0.050203	4.815808
241.908646	8000.586450	10.527232	-0.050200	4.815811
241.804162	8000.464125	10.532237	-0.050181	4.815776
241.849623	8000.600444	10.537242	-0.050189	4.815816
241.812080	8000.581690	10.542247	-0.050182	4.815810
241.765708	8000.488064	10.547251	-0.050174	4.815783
241.774901	8000.574687	10.552256	-0.050175	4.815808
241.812738	8000.553952	10.557261	-0.050182	4.815802
241.957544	8000.577654	10.562266	-0.050209	4.815808
241.715849	8000.592954	10.567271	-0.050164	4.815814
241.771199	8000.486032	10.572275	-0.050175	4.815783
241.801990	8000.607167	10.577280	-0.050181	4.815818
241.816070	8000.570034	10.582285	-0.050183	4.815807
241.991907	8000.485348	10.587290	-0.050216	4.815781
241.990015	8000.595278	10.592295	-0.050216	4.815813
241.607665	8000.572001	10.597299	-0.050145	4.815808
241.852812	8000.490574	10.602304	-0.050190	4.815784
241.606474	8000.567717	10.607309	-0.050144	4.815807
241.738151	8000.592273	10.612314	-0.050169	4.815814
241.900161	8000.581024	10.617319	-0.050199	4.815810
241.869354	8000.568785	10.622323	-0.050193	4.815806
241.933238	8000.486554	10.627328	-0.050205	4.815782
241.627462	8000.584084	10.632333	-0.050148	4.815812
241.594683	8000.573948	10.637338	-0.050142	4.815809
241.854995	8000.561090	10.642343	-0.050191	4.815804
241.772588	8000.545879	10.647347	-0.050176	4.815800
241.921357	8000.582455	10.652352	-0.050203	4.815810
241.868979	8000.475921	10.657357	-0.050193	4.815779
241.777019	8000.592931	10.662362	-0.050176	4.815814
241.669653	8000.500452	10.667367	-0.050156	4.815787
242.015276	8000.469761	10.672371	-0.050221	4.815777
242.175101	8000.596192	10.677376	-0.050251	4.815813
241.763856	8000.550027	10.682381	-0.050174	4.815801
241.761990	8000.495554	10.687386	-0.050174	4.815785
241.794296	8000.595363	10.692391	-0.050180	4.815814
241.688401	8000.576568	10.697395	-0.050160	4.815809
241.638422	8000.480749	10.702400	-0.050151	4.815782
241.750056	8000.573303	10.707405	-0.050172	4.815808
241.753364	8000.395079	10.712410	-0.050172	4.815756
241.717402	8000.583455	10.717415	-0.050166	4.815811
241.763972	8000.492403	10.722419	-0.050174	4.815784
241.986647	8000.581420	10.727424	-0.050216	4.815809
241.700114	8000.555426	10.732429	-0.050163	4.815803
241.746989	8000.602094	10.737434	-0.050171	4.815817
241.985898	8000.588889	10.742439	-0.050216	4.815812
241.873884	8000.484591	10.747443	-0.050195	4.815782
241.899492	8000.597102	10.752448	-0.050200	4.815814
241.853610	8000.572875	10.757453	-0.050191	4.815808
241.886855	8000.584092	10.762458	-0.050198	4.815811
241.817322	8000.476212	10.767463	-0.050185	4.815779
241.874140	8000.571081	10.772467	-0.050195	4.815807
242.031184	8000.608859	10.777472	-0.050225	4.815817
241.901215	8000.552309	10.782477	-0.050200	4.815801
241.881553	8000.484737	10.787482	-0.050197	4.815782
241.847259	8000.585602	10.792487	-0.050190	4.815811
241.755103	8000.563827	10.797491	-0.050173	4.815805
242.005393	8000.584969	10.802496	-0.050220	4.815810
241.980069	8000.548264	10.807501	-0.050215	4.815800
242.139552	8000.487866	10.812506	-0.050245	4.815781
241.950670	8000.563806	10.817511	-0.050210	4.815804
241.954825	8000.577754	10.822515	-0.050211	4.815808
242.139080	8000.588218	10.827520	-0.050245	4.815811
242.022048	8000.562837	10.832525	-0.050223	4.815804
241.828267	8000.489239	10.837530	-0.050187	4.815783
241.961831	8000.596028	10.842535	-0.050212	4.815814
241.861397	8000.589064	10.847539	-0.050193	4.815812
241.869134	8000.590260	10.852544	-0.050195	4.815813
241.683638	8000.499716	10.857549	-0.050160	4.815787
241.696756	8000.497796	10.862554	-0.050163	4.815786
241.716877	8000.478910	10.867559	-0.050167	4.815781
241.645435	8000.556753	10.872563	-0.050153	4.815804
241.784467	8000.591036	10.877568	-0.050179	4.815813
241.685066	8000.550995	10.882573	-0.050161	4.815802
241.765424	8000.574720	10.887578	-0.050176	4.815808
242.000904	8000.582811	10.892583	-0.050220	4.815810
241.857103	8000.570874	10.897587	-0.050193	4.815807
241.820047	8000.585222	10.902592	-0.050186	4.815811
241.835410	8000.473380	10.907597	-0.050189	4.815779
241.915518	8000.598518	10.912602	-0.050204	4.815815
241.869674	8000.466469	10.917607	-0.050195	4.815776
241.699811	8000.602499	10.922611	-0.050164	4.815817
241.910150	8000.406280	10.927616	-0.050203	4.815759
241.934619	8000.589231	10.932621	-0.050208	4.815812
241.790963	8000.393678	10.937626	-0.050181	4.815755
241.878321	8000.603269	10.942631	-0.050197	4.815816
242.061748	8000.573152	10.947635	-0.050231	4.815807
242.048422	8000.499277	10.952640	-0.050229	4.815785
241.867848	8000.574284	10.957645	-0.050195	4.815808
242.111772	8000.505648	10.962650	-0.050241	4.815787
241.903924	8000.581280	10.967655	-0.050202	4.815810
241.877607	8000.491181	10.972659	-0.050197	4.815784
241.951518	8000.598070	10.977664	-0.050211	4.815814
241.818918	8000.552153	10.982669	-0.050186	4.815802
241.798485	8000.569973	10.987674	-0.050183	4.815807
241.964297	8000.580137	10.992679	-0.050213	4.815809
241.991606	8000.550691	10.997683	-0.050219	4.815800
241.914016	8000.484315	11.002688	-0.050204	4.815781
241.924133	8000.546400	11.007693	-0.050206	4.815799
242.059516	8000.597706	11.012698	-0.050231	4.815814
241.866838	8000.478221	11.017703	-0.050195	4.815780
241.809974	8000.582990	11.022707	-0.050185	4.815811
242.003543	8000.589334	11.027712	-0.050221	4.815812
241.898626	8000.575892	11.032717	-0.050201	4.815808
241.930250	8000.578543	11.037722	-0.050207	4.815809
242.090388	8000.465846	11.042727	-0.050237	4.815775
242.157480	8000.574760	11.047731	-0.050250	4.815807
242.057158	8000.588082	11.052736	-0.050231	4.815811
241.772968	8000.543977	11.057741	-0.050178	4.815799
241.864479	8000.599909	11.062746	-0.050195	4.815815
242.040747	8000.564338	11.067751	-0.050228	4.815804
242.007380	8000.475192	11.072755	-0.050222	4.815778
242.305195	8000.585712	11.077760	-0.050277	4.815809
242.030567	8000.571654	11.082765	-0.050226	4.815806
242.123959	8000.583847	11.087770	-0.050244	4.815809
242.178292	8000.475839	11.092775	-0.050254	4.815778
242.179783	8000.599703	11.097779	-0.050254	4.815814
242.207010	8000.504067	11.102784	-0.050259	4.815786
241.892862	8000.568367	11.107789	-0.050201	4.815806
241.896108	8000.595112	11.112794	-0.050202	4.815814
241.799674	8000.478255	11.117799	-0.050184	4.815780
241.767154	8000.566338	11.122803	-0.050178	4.815806
242.007665	8000.589456	11.127808	-0.050222	4.815812
241.821028	8000.555474	11.132813	-0.050188	4.815803
241.854759	8000.584847	11.137818	-0.050194	4.815811
241.866919	8000.572236	11.142823	-0.050196	4.815807
241.881186	8000.556457	11.147827	-0.050199	4.815803
242.074685	8000.583084	11.152832	-0.050235	4.815809
241.992768	8000.472868	11.157837	-0.050220	4.815778
242.028805	8000.591953	11.162842	-0.050227	4.815812
242.252485	8000.513381	11.167847	-0.050268	4.815788
242.120615	8000.573164	11.172851	-0.050244	4.815806
242.247158	8000.575219	11.177856	-0.050267	4.815806
242.194189	8000.577565	11.182861	-0.050257	4.815807
242.176436	8000.578348	11.187866	-0.050254	4.815808
242.136636	8000.485895	11.192871	-0.050247	4.815781
241.904085	8000.605964	11.197875	-0.050204	4.815817
242.112635	8000.486579	11.202880	-0.050242	4.815781
241.876326	8000.579898	11.207885	-0.050198	4.815809
242.065894	8000.531732	11.212890	-0.050234	4.815794
242.115112	8000.545343	11.217895	-0.050243	4.815798
241.905070	8000.573967	11.222899	-0.050204	4.815808
242.178076	8000.512208	11.227904	-0.050255	4.815788
242.194199	8000.579728	11.232909	-0.050258	4.815808
242.069076	8000.493365	11.237914	-0.050234	4.815783
241.904850	8000.606001	11.242919	-0.050204	4.815817
241.789595	8000.484569	11.247923	-0.050182	4.815782
242.124419	8000.575405	11.252928	-0.050245	4.815807
241.820151	8000.556596	11.257933	-0.050188	4.815803
241.841120	8000.504629	11.262938	-0.050192	4.815788
241.825781	8000.594058	11.267943	-0.050189	4.815814
241.815202	8000.581078	11.272947	-0.050187	4.815810
241.976808	8000.573026	11.277952	-0.050218	4.815807
242.068527	8000.464557	11.282957	-0.050235	4.815775
241.965141	8000.582450	11.287962	-0.050215	4.815810
241.881855	8000.571494	11.292967	-0.050200	4.815807
242.038427	8000.556955	11.297971	-0.050229	4.815802
242.248111	8000.480291	11.302976	-0.050268	4.815779
242.175820	8000.591215	11.307981	-0.050255	4.815811
242.238518	8000.578356	11.312986	-0.050267	4.815807
242.319504	8000.587145	11.317991	-0.050282	4.815809
242.203947	8000.574599	11.322995	-0.050260	4.815806
242.190962	8000.590404	11.328000	-0.050258	4.815811
242.300308	8000.475816	11.333005	-0.050278	4.815777
242.203524	8000.586343	11.338010	-0.050260	4.815810
242.010618	8000.479665	11.343015	-0.050224	4.815779
242.039017	8000.565533	11.348019	-0.050230	4.815804
242.215322	8000.496868	11.353024	-0.050262	4.815784
241.939564	8000.595952	11.358029	-0.050211	4.815814
241.907429	8000.574083	11.363034	-0.050205	4.815808
242.132783	8000.578807	11.368039	-0.050247	4.815808
242.067501	8000.580954	11.373043	-0.050235	4.815809
241.987126	8000.494249	11.378048	-0.050220	4.815784
242.055026	8000.559406	11.383053	-0.050233	4.815803
242.078129	8000.593946	11.388058	-0.050237	4.815813
242.038748	8000.508973	11.393063	-0.050230	4.815788
242.223126	8000.476735	11.398067	-0.050264	4.815778
242.414829	8000.612225	11.403072	-0.050300	4.815816
242.363734	8000.483291	11.408077	-0.050290	4.815779
242.298004	8000.598593	11.413082	-0.050278	4.815813
242.292316	8000.498152	11.418087	-0.050277	4.815784
242.081646	8000.571603	11.423091	-0.050238	4.815806
242.072972	8000.508479	11.428096	-0.050236	4.815788
242.109151	8000.572055	11.433101	-0.050243	4.815806
241.948206	8000.577988	11.438106	-0.050213	4.815808
241.897112	8000.471475	11.443111	-0.050204	4.815778
241.930641	8000.543547	11.448115	-0.050210	4.815798
242.078737	8000.592924	11.453120	-0.050238	4.815812
242.019477	8000.573817	11.458125	-0.050227	4.815807
241.963521	8000.508859	11.463130	-0.050216	4.815788
242.075795	8000.590750	11.468135	-0.050237	4.815812
242.283570	8000.580243	11.473139	-0.050276	4.815808
242.304012	8000.506916	11.478144	-0.050280	4.815786
242.137240	8000.560795	11.483149	-0.050249	4.815803
242.387762	8000.590482	11.488154	-0.050295	4.815810
242.189958	8000.580871	11.493159	-0.050259	4.815808
242.140641	8000.550183	11.498163	-0.050249	4.815799
242.067317	8000.567145	11.503168	-0.050236	4.815805
241.870344	8000.559684	11.508173	-0.050199	4.815803
242.008751	8000.585417	11.513178	-0.050225	4.815810
242.158220	8000.601722	11.518183	-0.050253	4.815814
241.997226	8000.472075	11.523187	-0.050223	4.815777
241.991887	8000.593692	11.528192	-0.050222	4.815813
242.147512	8000.557787	11.533197	-0.050251	4.815802
242.313739	8000.576498	11.538202	-0.050282	4.815806
242.333755	8000.587501	11.543207	-0.050286	4.815809
242.215754	8000.591996	11.548211	-0.050264	4.815811
242.194674	8000.585251	11.553216	-0.050260	4.815809
242.085958	8000.549329	11.558221	-0.050240	4.815799
242.052026	8000.471918	11.563226	-0.050233	4.815777
242.081671	8000.561009	11.568231	-0.050239	4.815803
242.040098	8000.571013	11.573235	-0.050231	4.815806
242.253977	8000.583024	11.578240	-0.050271	4.815808
242.317120	8000.562700	11.583245	-0.050283	4.815802
242.291085	8000.594307	11.588250	-0.050278	4.815812
242.325729	8000.490251	11.593255	-0.050285	4.815781
242.179208	8000.574350	11.598259	-0.050257	4.815806
242.121359	8000.608644	11.603264	-0.050247	4.815817
242.022893	8000.570753	11.608269	-0.050228	4.815806
241.990762	8000.502979	11.613274	-0.050222	4.815786
242.249835	8000.589385	11.618279	-0.050271	4.815810
242.237123	8000.587046	11.623283	-0.050268	4.815810
242.153305	8000.488542	11.628288	-0.050253	4.815781
242.168504	8000.595547	11.633293	-0.050256	4.815813
242.307501	8000.512399	11.638298	-0.050281	4.815788
242.204819	8000.601479	11.643303	-0.050262	4.815814
242.098213	8000.561321	11.648307	-0.050243	4.815803
242.230624	8000.511161	11.653312	-0.050267	4.815788
242.020242	8000.502414	11.658317	-0.050228	4.815786
241.984298	8000.610725	11.663322	-0.050221	4.815818
242.177257	8000.507101	11.668327	-0.050257	4.815787
242.240235	8000.586057	11.673331	-0.050269	4.815809
242.327845	8000.498873	11.678336	-0.050285	4.815784
242.208666	8000.555659	11.683341	-0.050263	4.815801
242.153871	8000.585732	11.688346	-0.050253	4.815810
242.205195	8000.491554	11.693351	-0.050263	4.815782
242.081409	8000.592036	11.698355	-0.050240	4.815812
242.362875	8000.410847	11.703360	-0.050292	4.815758
242.302557	8000.566803	11.708365	-0.050281	4.815803
242.090079	8000.520658	11.713370	-0.050241	4.815791
242.063400	8000.504215	11.718375	-0.050236	4.815786
242.134979	8000.581175	11.723379	-0.050250	4.815808
242.274668	8000.517254	11.728384	-0.050276	4.815789
242.318108	8000.579880	11.733389	-0.050284	4.815807
242.253687	8000.575635	11.738394	-0.050272	4.815806
242.262130	8000.487167	11.743399	-0.050274	4.815780
242.138876	8000.585522	11.748403	-0.050251	4.815810
242.180952	8000.506140	11.753408	-0.050259	4.815786
242.333460	8000.582278	11.758413	-0.050287	4.815808
242.202952	8000.492624	11.763418	-0.050263	4.815782
242.197272	8000.517089	11.768423	-0.050262	4.815789
241.984154	8000.571284	11.773427	-0.050222	4.815806
242.229635	8000.604092	11.778432	-0.050268	4.815815
242.388111	8000.494570	11.783437	-0.050297	4.815782
242.402371	8000.585547	11.788442	-0.050300	4.815808
242.462228	8000.516061	11.793447	-0.050311	4.815788
242.263051	8000.591834	11.798451	-0.050274	4.815811
242.287066	8000.418214	11.803456	-0.050279	4.815760
242.361908	8000.513375	11.808461	-0.050293	4.815788
242.327618	8000.598227	11.813466	-0.050286	4.815813
242.414327	8000.581488	11.818471	-0.050302	4.815807
242.462421	8000.481919	11.823475	-0.050311	4.815778
242.382773	8000.606603	11.828480	-0.050297	4.815815
242.160636	8000.580585	11.833485	-0.050255	4.815808
242.374178	8000.516794	11.838490	-0.050295	4.815789
242.580086	8000.500919	11.843495	-0.050333	4.815783
242.178202	8000.587283	11.848499	-0.050259	4.815810
242.208778	8000.515188	11.853504	-0.050264	4.815789
242.235380	8000.552986	11.858509	-0.050269	4.815800
242.264194	8000.505416	11.863514	-0.050275	4.815786
242.436144	8000.595748	11.868519	-0.050307	4.815811
242.409596	8000.586779	11.873523	-0.050302	4.815809
242.389926	8000.513869	11.878528	-0.050298	4.815788
242.294219	8000.488833	11.883533	-0.050280	4.815781
242.411272	8000.597491	11.888538	-0.050302	4.815812
242.653642	8000.501072	11.893543	-0.050347	4.815783
242.461732	8000.573760	11.898547	-0.050312	4.815805
242.368686	8000.507133	11.903552	-0.050294	4.815786
242.369121	8000.543440	11.908557	-0.050295	4.815796
242.357217	8000.564601	11.913562	-0.050292	4.815803
242.300546	8000.359781	11.918567	-0.050282	4.815743
242.325563	8000.581174	11.923571	-0.050287	4.815808
242.374802	8000.513651	11.928576	-0.050296	4.815788
242.303481	8000.594700	11.933581	-0.050283	4.815812
242.282812	8000.597570	11.938586	-0.050279	4.815813
242.448807	8000.510589	11.943591	-0.050310	4.815786
242.259876	8000.480839	11.948595	-0.050274	4.815779
242.207027	8000.486391	11.953600	-0.050265	4.815780
242.437879	8000.574474	11.958605	-0.050308	4.815805
242.552319	8000.576333	11.963610	-0.050329	4.815805
242.538866	8000.591064	11.968615	-0.050327	4.815809
242.467428	8000.481016	11.973619	-0.050313	4.815778
242.397981	8000.595190	11.978624	-0.050300	4.815811
242.243567	8000.584148	11.983629	-0.050272	4.815809
242.165306	8000.477193	11.988634	-0.050257	4.815778
242.312448	8000.507338	11.993639	-0.050285	4.815786
242.233555	8000.595737	11.998643	-0.050270	4.815812
242.200087	8000.505522	12.003648	-0.050264	4.815786
242.124784	8000.593979	12.008653	-0.050250	4.815812
242.207096	8000.598519	12.013658	-0.050265	4.815813
242.259617	8000.499022	12.018663	-0.050275	4.815784
242.265086	8000.504452	12.023667	-0.050276	4.815785
242.416209	8000.601919	12.028672	-0.050304	4.815813
242.418886	8000.581681	12.033677	-0.050305	4.815807
242.356669	8000.486729	12.038682	-0.050293	4.815780
242.509945	8000.605582	12.043687	-0.050322	4.815814
242.471159	8000.515280	12.048691	-0.050314	4.815788
242.448874	8000.590719	12.053696	-0.050310	4.815810
242.572681	8000.573513	12.058701	-0.050334	4.815804
242.478908	8000.489793	12.063706	-0.050316	4.815780
242.520473	8000.601497	12.068711	-0.050324	4.815813
242.292621	8000.561507	12.073715	-0.050281	4.815802
242.492758	8000.510309	12.078720	-0.050319	4.815786
242.332109	8000.506639	12.083725	-0.050289	4.815786
242.253337	8000.605716	12.088730	-0.050274	4.815815
242.301431	8000.506147	12.093735	-0.050283	4.815786
242.325716	8000.509747	12.098739	-0.050288	4.815787
242.375394	8000.563933	12.103744	-0.050297	4.815802
242.418799	8000.516600	12.108749	-0.050305	4.815788
242.483181	8000.501633	12.113754	-0.050317	4.815784
242.488028	8000.489971	12.118759	-0.050318	4.815780
242.242255	8000.592745	12.123763	-0.050272	4.815811
242.359329	8000.515646	12.128768	-0.050294	4.815788
242.324156	8000.590876	12.133773	-0.050288	4.815810
242.364870	8000.481580	12.138778	-0.050295	4.815778
242.594868	8000.514136	12.143783	-0.050338	4.815787
242.419171	8000.595628	12.148787	-0.050306	4.815811
242.311439	8000.510613	12.153792	-0.050285	4.815787
242.310557	8000.578926	12.158797	-0.050285	4.815807
242.422448	8000.508149	12.163802	-0.050306	4.815786
242.319080	8000.590813	12.168807	-0.050287	4.815810
242.171016	8000.539307	12.173811	-0.050259	4.815796
242.439737	8000.593843	12.178816	-0.050310	4.815811
242.600984	8000.561231	12.183821	-0.050340	4.815800
242.437707	8000.567126	12.188826	-0.050309	4.815803
242.452292	8000.497974	12.193831	-0.050312	4.815783
242.474100	8000.573060	12.198835	-0.050316	4.815804
242.347331	8000.508020	12.203840	-0.050292	4.815786
242.540264	8000.553855	12.208845	-0.050328	4.815798
242.563472	8000.558504	12.213850	-0.050333	4.815800
242.499949	8000.514774	12.218855	-0.050321	4.815787
242.620879	8000.586130	12.223859	-0.050344	4.815808
242.658591	8000.496001	12.228864	-0.050351	4.815781
242.618564	8000.595706	12.233869	-0.050343	4.815810
242.334594	8000.473671	12.238874	-0.050290	4.815776
242.444581	8000.512822	12.243879	-0.050311	4.815787
242.306555	8000.594925	12.248883	-0.050285	4.815812
242.246168	8000.508543	12.253888	-0.050274	4.815787
242.241630	8000.581066	12.258893	-0.050273	4.815808
242.300709	8000.576689	12.263898	-0.050284	4.815806
242.468463	8000.496142	12.268903	-0.050315	4.815782
242.183203	8000.540627	12.273907	-0.050262	4.815796
242.434286	8000.559648	12.278912	-0.050309	4.815801
242.474506	8000.568843	12.283917	-0.050317	4.815803
242.429797	8000.584135	12.288922	-0.050308	4.815808
242.594436	8000.405321	12.293927	-0.050339	4.815755
242.407479	8000.575238	12.298931	-0.050304	4.815805
242.459454	8000.504556	12.303936	-0.050314	4.815784
242.323445	8000.586691	12.308941	-0.050289	4.815809
242.444958	8000.469097	12.313946	-0.050311	4.815774
242.286068	8000.606374	12.318951	-0.050282	4.815815
242.450600	8000.480937	12.323955	-0.050312	4.815778
242.519776	8000.615508	12.328960	-0.050325	4.815817
242.546493	8000.485701	12.333965	-0.050330	4.815779
242.480613	8000.531608	12.338970	-0.050318	4.815792
242.516642	8000.563155	12.343975	-0.050325	4.815801
242.484751	8000.546627	12.348979	-0.050319	4.815797
242.520892	8000.583513	12.353984	-0.050326	4.815807
242.514819	8000.465985	12.358989	-0.050325	4.815773
242.575657	8000.595083	12.363994	-0.050336	4.815810
242.541969	8000.605215	12.368999	-0.050330	4.815813
242.359815	8000.555290	12.374003	-0.050296	4.815800
242.485370	8000.495410	12.379008	-0.050319	4.815782
242.590593	8000.593201	12.384013	-0.050339	4.815810
242.492925	8000.596957	12.389018	-0.050321	4.815811
242.619804	8000.525355	12.394023	-0.050344	4.815790
242.529594	8000.531368	12.399027	-0.050328	4.815792
242.663974	8000.577321	12.404032	-0.050353	4.815805
242.507448	8000.473366	12.409037	-0.050324	4.815775
242.317317	8000.584515	12.414042	-0.050288	4.815808
242.553797	8000.591556	12.419047	-0.050332	4.815809
242.274225	8000.560335	12.424051	-0.050280	4.815802
242.357637	8000.579839	12.429056	-0.050296	4.815807
242.576307	8000.578051	12.434061	-0.050337	4.815805
242.538090	8000.572096	12.439066	-0.050329	4.815804
242.525494	8000.506772	12.444071	-0.050327	4.815785
242.570674	8000.596116	12.449075	-0.050336	4.815811
242.602492	8000.505892	12.454080	-0.050342	4.815784
242.436222	8000.603550	12.459085	-0.050311	4.815813
242.283222	8000.495382	12.464090	-0.050282	4.815783
242.696000	8000.612039	12.469095	-0.050359	4.815815
242.427179	8000.488114	12.474099	-0.050309	4.815780
242.452760	8000.518423	12.479104	-0.050314	4.815789
242.605077	8000.589221	12.484109	-0.050342	4.815808
242.468630	8000.579538	12.489114	-0.050317	4.815806
242.630927	8000.501037	12.494119	-0.050347	4.815783
242.639664	8000.590858	12.499123	-0.050349	4.815809
242.568375	8000.490420	12.504128	-0.050335	4.815780
242.668605	8000.502724	12.509133	-0.050354	4.815783
242.524097	8000.587924	12.514138	-0.050327	4.815808
242.664505	8000.513339	12.519143	-0.050353	4.815786
242.573637	8000.483044	12.524147	-0.050337	4.815778
242.455255	8000.611370	12.529152	-0.050315	4.815816
242.669789	8000.518771	12.534157	-0.050355	4.815788
242.674198	8000.490021	12.539162	-0.050355	4.815779
242.576703	8000.609078	12.544167	-0.050337	4.815814
242.474105	8000.486781	12.549171	-0.050318	4.815779
242.577123	8000.510874	12.554176	-0.050337	4.815786
242.468378	8000.573167	12.559181	-0.050317	4.815804
242.410132	8000.586104	12.564186	-0.050306	4.815808
242.534156	8000.492036	12.569191	-0.050330	4.815780
242.561791	8000.496758	12.574195	-0.050335	4.815782
242.362456	8000.378231	12.579200	-0.050298	4.815748
242.296760	8000.566127	12.584205	-0.050285	4.815803
242.368192	8000.497897	12.589210	-0.050299	4.815783
242.433506	8000.605716	12.594215	-0.050311	4.815814
242.481551	8000.475186	12.599219	-0.050320	4.815776
242.447983	8000.615564	12.604224	-0.050314	4.815817
242.606239	8000.501768	12.609229	-0.050343	4.815783
242.500611	8000.594004	12.614234	-0.050324	4.815810
242.532942	8000.506990	12.619239	-0.050330	4.815785
242.427302	8000.497807	12.624243	-0.050310	4.815783
242.526437	8000.613648	12.629248	-0.050329	4.815816
242.587883	8000.501484	12.634253	-0.050340	4.815783
242.680636	8000.494451	12.639258	-0.050357	4.815780
242.734057	8000.609551	12.644263	-0.050367	4.815814
242.579148	8000.485337	12.649267	-0.050338	4.815778
242.587693	8000.614655	12.654272	-0.050340	4.815816
242.636188	8000.490538	12.659277	-0.050349	4.815779
242.453751	8000.596475	12.664282	-0.050315	4.815811
242.563277	8000.520321	12.669287	-0.050336	4.815789
242.643631	8000.582479	12.674291	-0.050351	4.815806
242.442014	8000.584549	12.679296	-0.050313	4.815808
242.489768	8000.582124	12.684301	-0.050322	4.815807
242.456614	8000.506859	12.689306	-0.050316	4.815785
242.528230	8000.513361	12.694311	-0.050329	4.815787
242.397285	8000.585970	12.699315	-0.050305	4.815808
242.797027	8000.519861	12.704320	-0.050379	4.815787
242.744622	8000.398378	12.709325	-0.050370	4.815752
242.539525	8000.601096	12.714330	-0.050332	4.815812
242.522951	8000.504749	12.719335	-0.050328	4.815784
242.634633	8000.501225	12.724339	-0.050349	4.815783
242.685014	8000.511653	12.729344	-0.050359	4.815785
242.741664	8000.482682	12.734349	-0.050369	4.815777
242.521458	8000.518614	12.739354	-0.050328	4.815788
242.612433	8000.510484	12.744359	-0.050345	4.815785
242.394671	8000.589158	12.749363	-0.050305	4.815809
242.424091	8000.510638	12.754368	-0.050310	4.815786
242.708137	8000.565423	12.759373	-0.050363	4.815801
242.443849	8000.583559	12.764378	-0.050314	4.815808
242.791078	8000.520868	12.769383	-0.050379	4.815788
242.641387	8000.589971	12.774387	-0.050351	4.815808
242.753948	8000.514934	12.779392	-0.050372	4.815786
242.692536	8000.496859	12.784397	-0.050360	4.815781
242.698323	8000.590903	12.789402	-0.050362	4.815808
242.813346	8000.515905	12.794407	-0.050383	4.815786
242.620228	8000.582168	12.799411	-0.050347	4.815806
242.556870	8000.506414	12.804416	-0.050335	4.815784
242.547946	8000.597015	12.809421	-0.050334	4.815811
242.483135	8000.494548	12.814426	-0.050322	4.815781
242.569104	8000.584553	12.819431	-0.050338	4.815807
242.668129	8000.574419	12.824435	-0.050356	4.815804
242.649455	8000.501524	12.829440	-0.050353	4.815783
242.887764	8000.487242	12.834445	-0.050397	4.815777
242.597262	8000.592494	12.839450	-0.050343	4.815809
242.632478	8000.504459	12.844455	-0.050350	4.815784
242.626675	8000.594044	12.849459	-0.050349	4.815810
242.615041	8000.500979	12.854464	-0.050346	4.815783
242.559490	8000.597230	12.859469	-0.050336	4.815811
242.595739	8000.513483	12.864474	-0.050343	4.815786
242.767521	8000.539758	12.869479	-0.050375	4.815793
242.726314	8000.564714	12.874483	-0.050367	4.815801
242.796009	8000.498590	12.879488	-0.050380	4.815781
242.664551	8000.582935	12.884493	-0.050356	4.815806
242.441108	8000.585719	12.889498	-0.050314	4.815808
242.620303	8000.492546	12.894503	-0.050348	4.815780
242.511022	8000.610345	12.899507	-0.050327	4.815815
242.526621	8000.505979	12.904512	-0.050330	4.815784
242.630717	8000.409453	12.909517	-0.050350	4.815756
242.385823	8000.582701	12.914522	-0.050304	4.815808
242.635128	8000.503476	12.919527	-0.050351	4.815783
242.630866	8000.497005	12.924531	-0.050350	4.815781
242.567171	8000.517326	12.929536	-0.050338	4.815788
242.768207	8000.598522	12.934541	-0.050376	4.815810
242.769682	8000.494994	12.939546	-0.050376	4.815780
242.750189	8000.528843	12.944551	-0.050372	4.815790
242.593249	8000.580747	12.949555	-0.050343	4.815806
242.736689	8000.590549	12.954560	-0.050370	4.815808
242.794334	8000.598960	12.959565	-0.050381	4.815810
242.714929	8000.579526	12.964570	-0.050366	4.815805
242.858428	8000.504990	12.969575	-0.050392	4.815783
242.920572	8000.582867	12.974579	-0.050404	4.815805
242.760604	8000.504477	12.979584	-0.050374	4.815783
242.516492	8000.596602	12.984589	-0.050329	4.815811
242.474906	8000.497714	12.989594	-0.050321	4.815782
242.733631	8000.518994	12.994599	-0.050369	4.815787
242.622259	8000.575907	12.999603	-0.050349	4.815804
242.535331	8000.602257	13.004608	-0.050333	4.815813
242.833687	8000.505679	13.009613	-0.050388	4.815783
242.660326	8000.601087	13.014618	-0.050356	4.815812
242.826815	8000.492762	13.019623	-0.050387	4.815779
242.657431	8000.566883	13.024627	-0.050355	4.815802
242.664591	8000.568070	13.029632	-0.050357	4.815802
242.755734	8000.504429	13.034637	-0.050374	4.815783
242.846268	8000.599847	13.039642	-0.050391	4.815810
242.819244	8000.412585	13.044647	-0.050386	4.815756
242.458587	8000.569010	13.049651	-0.050319	4.815803
242.813443	8000.602525	13.054656	-0.050385	4.815811
242.986354	8000.508183	13.059661	-0.050417	4.815783
242.586561	8000.588175	13.064666	-0.050343	4.815808
242.633941	8000.602825	13.069671	-0.050351	4.815812
242.443236	8000.488707	13.074675	-0.050316	4.815780
242.517767	8000.485648	13.079680	-0.050330	4.815779
242.563733	8000.582478	13.084685	-0.050338	4.815807
242.624140	8000.580258	13.089690	-0.050350	4.815806
242.792481	8000.481571	13.094695	-0.050381	4.815776
242.616230	8000.534229	13.099699	-0.050348	4.815792
242.713287	8000.599861	13.104704	-0.050366	4.815811
242.822603	8000.501284	13.109709	-0.050387	4.815782
242.794136	8000.584097	13.114714	-0.050381	4.815806
242.799275	8000.496641	13.119719	-0.050382	4.815780
242.650348	8000.602054	13.124723	-0.050355	4.815812
242.661864	8000.511499	13.129728	-0.050357	4.815785
242.748202	8000.510767	13.134733	-0.050373	4.815785
242.652577	8000.499611	13.139738	-0.050355	4.815782
242.693224	8000.506679	13.144743	-0.050363	4.815784
242.536490	8000.582072	13.149747	-0.050334	4.815807
242.739613	8000.501031	13.154752	-0.050372	4.815782
242.681064	8000.488341	13.159757	-0.050361	4.815779
242.523484	8000.603221	13.164762	-0.050331	4.815813
242.618848	8000.389121	13.169767	-0.050349	4.815750
242.702522	8000.490832	13.174771	-0.050365	4.815779
242.717141	8000.494275	13.179776	-0.050367	4.815780
242.867314	8000.571444	13.184781	-0.050396	4.815802
242.606192	8000.575752	13.189786	-0.050347	4.815804
242.968646	8000.594445	13.194791	-0.050414	4.815808
242.914284	8000.567944	13.199795	-0.050404	4.815801
242.844642	8000.505965	13.204800	-0.050391	4.815783
242.807287	8000.590768	13.209805	-0.050385	4.815808
242.806543	8000.582218	13.214810	-0.050384	4.815805
242.650988	8000.605320	13.219815	-0.050355	4.815813
242.694344	8000.474714	13.224819	-0.050364	4.815774
242.753947	8000.604860	13.229824	-0.050375	4.815812
242.635575	8000.520740	13.234829	-0.050353	4.815788
242.600997	8000.590641	13.239834	-0.050346	4.815809
242.890251	8000.504592	13.244839	-0.050400	4.815782
242.627491	8000.595347	13.249843	-0.050351	4.815810
242.599731	8000.513764	13.254848	-0.050346	4.815786
242.665348	8000.602372	13.259853	-0.050358	4.815812
242.635469	8000.504741	13.264858	-0.050353	4.815784
242.765380	8000.480161	13.269863	-0.050377	4.815776
242.640680	8000.512304	13.274867	-0.050354	4.815786
242.794947	8000.594877	13.279872	-0.050383	4.815809
242.837215	8000.513362	13.284877	-0.050391	4.815785
242.700229	8000.567724	13.289882	-0.050365	4.815802
242.847433	8000.534885	13.294887	-0.050393	4.815791
242.789708	8000.578790	13.299891	-0.050382	4.815804
242.558095	8000.513116	13.304896	-0.050339	4.815786
242.536241	8000.600306	13.309901	-0.050335	4.815812
242.751396	8000.502378	13.314906	-0.050375	4.815782
242.881985	8000.605920	13.319911	-0.050399	4.815812
242.800135	8000.513850	13.324915	-0.050384	4.815785
242.800649	8000.505321	13.329920	-0.050384	4.815783
242.774471	8000.375723	13.334925	-0.050379	4.815745
242.461484	8000.505164	13.339930	-0.050321	4.815784
242.848296	8000.517845	13.344935	-0.050393	4.815786
242.872275	8000.564143	13.349939	-0.050398	4.815800
242.789169	8000.599095	13.354944	-0.050382	4.815810
242.831290	8000.499429	13.359949	-0.050390	4.815781
242.812856	8000.589877	13.364954	-0.050387	4.815808
242.882986	8000.609166	13.369959	-0.050400	4.815813
242.809003	8000.492670	13.374963	-0.050386	4.815779
242.905424	8000.605265	13.379968	-0.050404	4.815812
242.856186	8000.507320	13.384973	-0.050395	4.815783
242.713321	8000.579736	13.389978	-0.050368	4.815805
242.778638	8000.507135	13.394983	-0.050380	4.815784
242.879148	8000.499160	13.399987	-0.050399	4.815781
242.609857	8000.509741	13.404992	-0.050349	4.815785
242.672476	8000.519300	13.409997	-0.050361	4.815788
242.763837	8000.602988	13.415002	-0.050378	4.815812
242.702350	8000.598791	13.420007	-0.050366	4.815811
242.676902	8000.462799	13.425011	-0.050362	4.815771
242.943808	8000.504496	13.430016	-0.050411	4.815782
242.973715	8000.586120	13.435021	-0.050417	4.815806
242.961755	8000.578455	13.440026	-0.050415	4.815803
243.007671	8000.509810	13.445031	-0.050423	4.815783
242.908510	8000.588273	13.450035	-0.050405	4.815807
242.961377	8000.599809	13.455040	-0.050415	4.815810
242.836901	8000.538008	13.460045	-0.050392	4.815792
242.832284	8000.535801	13.465050	-0.050391	4.815792
242.775333	8000.597867	13.470055	-0.050380	4.815810
242.707854	8000.501761	13.475059	-0.050368	4.815782
242.846774	8000.515760	13.480064	-0.050394	4.815786
242.910010	8000.483694	13.485069	-0.050405	4.815776
242.631479	8000.506936	13.490074	-0.050354	4.815784
242.740911	8000.464943	13.495079	-0.050374	4.815771
243.018180	8000.495065	13.500083	-0.050426	4.815779
242.864533	8000.601469	13.505088	-0.050397	4.815811
242.856884	8000.514873	13.510093	-0.050396	4.815785
242.848524	8000.511538	13.515098	-0.050394	4.815784
243.047049	8000.516896	13.520103	-0.050431	4.815785
242.784224	8000.498757	13.525107	-0.050382	4.815781
242.684075	8000.530231	13.530112	-0.050364	4.815791
242.895267	8000.516577	13.535117	-0.050403	4.815786
242.737575	8000.603699	13.540122	-0.050374	4.815812
242.750696	8000.421359	13.545127	-0.050376	4.815759
242.839093	8000.603216	13.550131	-0.050393	4.815811
242.630623	8000.504823	13.555136	-0.050354	4.815784
242.718612	8000.601268	13.560141	-0.050370	4.815811
242.712610	8000.485875	13.565146	-0.050369	4.815778
243.027078	8000.516600	13.570151	-0.050428	4.815785
242.816291	8000.443791	13.575155	-0.050388	4.815765
242.707030	8000.586145	13.580160	-0.050368	4.815807
243.112112	8000.513717	13.585165	-0.050444	4.815784
242.853419	8000.497780	13.590170	-0.050395	4.815780
242.863548	8000.594030	13.595175	-0.050397	4.815808
242.889195	8000.575232	13.600179	-0.050402	4.815803
242.913828	8000.464606	13.605184	-0.050407	4.815770
242.900963	8000.550874	13.610189	-0.050404	4.815796
242.799646	8000.489449	13.615194	-0.050386	4.815778
243.029116	8000.493174	13.620199	-0.050428	4.815778
242.947716	8000.497194	13.625203	-0.050413	4.815780
242.881657	8000.609289	13.630208	-0.050401	4.815813
242.946850	8000.504659	13.635213	-0.050413	4.815782
243.010753	8000.596443	13.640218	-0.050425	4.815808
242.819636	8000.405452	13.645223	-0.050389	4.815754
242.750444	8000.596496	13.650227	-0.050377	4.815810
242.787431	8000.504219	13.655232	-0.050384	4.815783
242.710578	8000.504043	13.660237	-0.050369	4.815783
242.769391	8000.575460	13.665242	-0.050380	4.815803
242.823709	8000.411937	13.670247	-0.050390	4.815755
242.809920	8000.612421	13.675251	-0.050388	4.815814
242.821492	8000.513326	13.680256	-0.050390	4.815785
242.986458	8000.503194	13.685261	-0.050421	4.815781
242.818687	8000.490867	13.690266	-0.050390	4.815779
242.939916	8000.618811	13.695271	-0.050412	4.815815
242.944546	8000.497184	13.700275	-0.050413	4.815780
242.870268	8000.494915	13.705280	-0.050399	4.815779
243.113128	8000.520208	13.710285	-0.050445	4.815786
243.016063	8000.576286	13.715290	-0.050427	4.815803
243.194689	8000.488442	13.720295	-0.050460	4.815776
243.069297	8000.583561	13.725299	-0.050437	4.815804
242.752274	8000.488745	13.730304	-0.050378	4.815778
242.840806	8000.594806	13.735309	-0.050394	4.815809
242.864800	8000.591995	13.740314	-0.050399	4.815808
242.957852	8000.514506	13.745319	-0.050416	4.815785
242.776253	8000.575618	13.750323	-0.050382	4.815803
242.946338	8000.502582	13.755328	-0.050414	4.815781
242.825407	8000.498488	13.760333	-0.050391	4.815781
242.925716	8000.585524	13.765338	-0.050410	4.815806
243.017728	8000.513356	13.770343	-0.050427	4.815784
242.798278	8000.498056	13.775347	-0.050386	4.815781
242.988389	8000.474453	13.780352	-0.050422	4.815773
242.968028	8000.501883	13.785357	-0.050418	4.815781
243.020572	8000.575334	13.790362	-0.050428	4.815802
242.898907	8000.526389	13.795367	-0.050405	4.815789
242.797658	8000.535425	13.800371	-0.050386	4.815792
242.759161	8000.557223	13.805376	-0.050379	4.815798
242.881369	8000.360639	13.810381	-0.050402	4.815740
242.649708	8000.503142	13.815386	-0.050359	4.815783
242.801789	8000.506679	13.820391	-0.050387	4.815783
243.003300	8000.549451	13.825395	-0.050425	4.815795
242.943026	8000.558084	13.830400	-0.050414	4.815798
242.990799	8000.498010	13.835405	-0.050423	4.815780
242.716302	8000.566155	13.840410	-0.050372	4.815801
242.785706	8000.590771	13.845415	-0.050385	4.815808
242.776676	8000.546856	13.850419	-0.050383	4.815795
242.936848	8000.499281	13.855424	-0.050413	4.815780
242.935951	8000.512080	13.860429	-0.050413	4.815784
242.832048	8000.485843	13.865434	-0.050393	4.815777
243.084421	8000.375708	13.870439	-0.050440	4.815744
243.017685	8000.606294	13.875443	-0.050428	4.815811
242.942923	8000.495123	13.880448	-0.050414	4.815779
242.975956	8000.619501	13.885453	-0.050420	4.815815
243.233168	8000.474214	13.890458	-0.050468	4.815772
242.900114	8000.603330	13.895463	-0.050406	4.815811
243.007237	8000.584787	13.900467	-0.050426	4.815805
242.877336	8000.598696	13.905472	-0.050402	4.815810
243.172092	8000.512735	13.910477	-0.050457	4.815783
242.980601	8000.495753	13.915482	-0.050421	4.815779
242.984199	8000.504355	13.920487	-0.050422	4.815782
243.030288	8000.603323	13.925491	-0.050431	4.815810
242.933095	8000.501397	13.930496	-0.050412	4.815781
242.920058	8000.614352	13.935501	-0.050410	4.815814
242.972665	8000.482828	13.940506	-0.050420	4.815775
243.189917	8000.609127	13.945511	-0.050460	4.815811
243.124350	8000.490631	13.950515	-0.050448	4.815777
242.949271	8000.605228	13.955520	-0.050416	4.815811
243.048060	8000.490467	13.960525	-0.050434	4.815777
242.859320	8000.510895	13.965530	-0.050399	4.815784
243.124100	8000.486368	13.970535	-0.050448	4.815776
242.994299	8000.478928	13.975539	-0.050424	4.815774
242.737138	8000.586855	13.980544	-0.050376	4.815807
242.858486	8000.508758	13.985549	-0.050399	4.815784
243.033313	8000.495582	13.990554	-0.050432	4.815779
243.023018	8000.446310	13.995559	-0.050430	4.815764
242.959810	8000.462368	14.000563	-0.050418	4.815769
243.022381	8000.597902	14.005568	-0.050430	4.815809
243.133935	8000.533524	14.010573	-0.050450	4.815789
242.845696	8000.553405	14.015578	-0.050397	4.815797
242.879671	8000.610541	14.020583	-0.050403	4.815813
243.170801	8000.505305	14.025587	-0.050457	4.815781
243.064398	8000.601800	14.030592	-0.050438	4.815810
243.181566	8000.520432	14.035597	-0.050459	4.815785
242.885894	8000.493219	14.040602	-0.050404	4.815779
242.981532	8000.417907	14.045607	-0.050422	4.815756
243.057336	8000.515222	14.050611	-0.050436	4.815784
242.736740	8000.490808	14.055616	-0.050377	4.815779
242.851775	8000.435028	14.060621	-0.050398	4.815762
242.724149	8000.577083	14.065626	-0.050374	4.815804
242.880508	8000.526243	14.070631	-0.050404	4.815789
242.901129	8000.439039	14.075635	-0.050407	4.815763
242.752984	8000.560478	14.080640	-0.050380	4.815799
242.933978	8000.394739	14.085645	-0.050414	4.815750
243.032012	8000.518036	14.090650	-0.050432	4.815785
243.075566	8000.405582	14.095655	-0.050440	4.815752
242.940837	8000.406602	14.100659	-0.050415	4.815753
242.988083	8000.511994	14.105664	-0.050424	4.815784
243.052516	8000.467136	14.110669	-0.050436	4.815770
242.898802	8000.443294	14.115674	-0.050407	4.815764
242.876078	8000.382077	14.120679	-0.050403	4.815746
242.739258	8000.509037	14.125683	-0.050378	4.815784
242.894191	8000.513688	14.130688	-0.050407	4.815785
242.844345	8000.342070	14.135693	-0.050397	4.815735
242.790621	8000.515216	14.140698	-0.050387	4.815786
242.882573	8000.504967	14.145703	-0.050404	4.815782
242.938388	8000.407658	14.150707	-0.050415	4.815754
242.751082	8000.467610	14.155712	-0.050380	4.815772
243.028016	8000.293819	14.160717	-0.050431	4.815720
243.054627	8000.523782	14.165722	-0.050437	4.815787
243.025021	8000.318330	14.170727	-0.050431	4.815727
243.065029	8000.433212	14.175731	-0.050439	4.815760
242.894862	8000.446469	14.180736	-0.050407	4.815765
242.872282	8000.441835	14.185741	-0.050403	4.815764
242.784830	8000.513015	14.190746	-0.050387	4.815785
242.875783	8000.421614	14.195751	-0.050403	4.815758
242.836919	8000.435932	14.200755	-0.050396	4.815762
242.978574	8000.566342	14.205760	-0.050423	4.815800
243.081241	8000.518901	14.210765	-0.050442	4.815785
242.960721	8000.509476	14.215770	-0.050419	4.815783
242.954022	8000.390869	14.220775	-0.050418	4.815749
242.974458	8000.499029	14.225779	-0.050422	4.815780
242.956469	8000.499807	14.230784	-0.050419	4.815780
243.116242	8000.176791	14.235789	-0.050448	4.815685
242.857408	8000.328462	14.240794	-0.050400	4.815731
243.044467	8000.428647	14.245799	-0.050435	4.815759
243.121152	7999.518206	14.250803	-0.050449	4.815493

242.993033	7996.238114	14.255808	-0.050423	4.814534
243.101532	7990.714279	14.260813	-0.050440	4.812917
243.004917	7983.949698	14.265818	-0.050417	4.810938
243.005878	7976.642584	14.270823	-0.050413	4.808798
242.896168	7969.046125	14.275827	-0.050387	4.806574
242.685715	7961.235490	14.280832	-0.050343	4.804285
242.486243	7953.386249	14.285837	-0.050301	4.801985
242.628584	7945.356551	14.290842	-0.050322	4.799629
242.625850	7937.458362	14.295847	-0.050317	4.797311
242.378487	7929.414830	14.300851	-0.050265	4.794950
242.298332	7921.345882	14.305856	-0.050245	4.792580
242.441389	7913.358446	14.310861	-0.050267	4.790231
242.505948	7905.410936	14.315866	-0.050273	4.787894
242.300006	7897.404173	14.320871	-0.050230	4.785539
242.211021	7889.417864	14.325875	-0.050208	4.783188
242.152581	7881.372343	14.330880	-0.050192	4.780819
242.150454	7873.413145	14.335885	-0.050187	4.778474
242.137382	7865.406903	14.340890	-0.050179	4.776113
242.133324	7857.400514	14.345895	-0.050173	4.773752
241.993591	7849.369950	14.350899	-0.050142	4.771383
241.972081	7841.319527	14.355904	-0.050133	4.769006
241.965354	7833.431810	14.360909	-0.050126	4.766676
241.810545	7825.337076	14.365914	-0.050092	4.764284
241.752357	7817.421784	14.370919	-0.050076	4.761944
241.780517	7809.379532	14.375923	-0.050076	4.759565
241.675285	7801.409378	14.380928	-0.050051	4.757206
241.733139	7793.371273	14.385933	-0.050057	4.754825
241.548255	7785.358736	14.390938	-0.050017	4.752452
241.649860	7777.238610	14.395943	-0.050031	4.750045
241.624695	7769.356964	14.400947	-0.050021	4.747707
241.425327	7761.305942	14.405952	-0.049979	4.745319
241.519851	7753.359842	14.410957	-0.049991	4.742960
241.533224	7745.343296	14.415962	-0.049989	4.740579
241.254516	7737.340508	14.420967	-0.049932	4.738201
241.420239	7729.329345	14.425971	-0.049957	4.735819
241.338808	7721.288345	14.430976	-0.049937	4.733427
241.464026	7713.307896	14.435981	-0.049955	4.731051
241.218396	7705.308135	14.440986	-0.049904	4.728670
241.209404	7697.356514	14.445991	-0.049897	4.726301
241.213179	7689.312668	14.450995	-0.049893	4.723903
241.117254	7681.318116	14.456000	-0.049870	4.721519
241.285625	7673.321472	14.461005	-0.049896	4.719133
241.081498	7665.380165	14.466010	-0.049853	4.716763
241.057621	7657.339863	14.471015	-0.049843	4.714361
241.021144	7649.261801	14.476019	-0.049831	4.711947
240.863560	7641.278854	14.481024	-0.049797	4.709561
240.815172	7633.340472	14.486029	-0.049782	4.707186
240.740576	7625.277664	14.491034	-0.049763	4.704773
240.738295	7617.324806	14.496039	-0.049758	4.702392
240.688596	7609.326702	14.501043	-0.049743	4.699996
240.464729	7601.299283	14.506048	-0.049696	4.697590
240.586324	7593.320939	14.511053	-0.049714	4.695197
240.544644	7585.299849	14.516058	-0.049701	4.692790
240.459660	7577.248331	14.521063	-0.049680	4.690373
240.490297	7569.306623	14.526067	-0.049680	4.687987
240.449953	7561.278201	14.531072	-0.049668	4.685575
240.457402	7553.337240	14.536077	-0.049664	4.683187
240.201012	7545.275499	14.541082	-0.049611	4.680762
240.116743	7537.296676	14.546087	-0.049590	4.678361
240.246850	7529.348933	14.551091	-0.049609	4.675967
240.189438	7521.241717	14.556096	-0.049593	4.673524
240.076486	7513.164408	14.561101	-0.049567	4.671090
239.929472	7505.215397	14.566106	-0.049534	4.668692
239.951607	7497.202953	14.571111	-0.049533	4.666274
239.891573	7489.216055	14.576115	-0.049517	4.663863
239.862985	7481.264431	14.581120	-0.049507	4.661461
239.891555	7473.239672	14.586125	-0.049507	4.659035
239.773641	7465.247511	14.591130	-0.049480	4.656618
239.831049	7457.232238	14.596135	-0.049485	4.654193
239.875513	7449.262334	14.601139	-0.049488	4.651781
239.667878	7441.185616	14.606144	-0.049444	4.649335
239.470503	7433.238918	14.611149	-0.049402	4.646927
239.553395	7425.180741	14.616154	-0.049413	4.644483
239.351108	7417.282573	14.621159	-0.049370	4.642087
239.305622	7409.233587	14.626163	-0.049356	4.639644
239.181202	7401.274038	14.631168	-0.049328	4.637227
239.301191	7393.230722	14.636173	-0.049345	4.634784
239.192228	7385.181041	14.641178	-0.049319	4.632336
239.221772	7377.155317	14.646183	-0.049320	4.629895
239.212058	7369.207632	14.651187	-0.049313	4.627477
239.257157	7361.146269	14.656192	-0.049316	4.625022
239.064093	7353.225311	14.661197	-0.049275	4.622609
239.072491	7345.192930	14.666202	-0.049271	4.620161
239.210733	7337.196560	14.671207	-0.049292	4.617722
239.193726	7329.214604	14.676211	-0.049283	4.615287
238.965030	7321.152066	14.681216	-0.049236	4.612826
238.895664	7313.181739	14.686221	-0.049218	4.610391
238.736985	7305.174861	14.691226	-0.049183	4.607944
238.770770	7297.172150	14.696231	-0.049184	4.605497
238.847099	7289.200170	14.701235	-0.049193	4.603058
238.616410	7281.175661	14.706240	-0.049145	4.600602
238.543766	7273.206271	14.711245	-0.049126	4.598161
238.549945	7265.194170	14.716250	-0.049122	4.595706
238.511966	7257.155895	14.721255	-0.049110	4.593241
238.353735	7249.111002	14.726259	-0.049075	4.590773
238.370691	7241.088431	14.731264	-0.049073	4.588311
238.515974	7233.116618	14.736269	-0.049095	4.585863
238.384753	7225.153782	14.741274	-0.049065	4.583416
238.097470	7217.145938	14.746279	-0.049007	4.580954
238.241882	7209.175751	14.751283	-0.049029	4.578503
238.101197	7201.132585	14.756288	-0.048997	4.576027
238.105355	7193.144035	14.761293	-0.048993	4.573568
237.974705	7185.100492	14.766298	-0.048963	4.571089
238.050502	7177.108192	14.771303	-0.048972	4.568626
238.081633	7169.130476	14.776307	-0.048973	4.566165
237.890286	7161.115489	14.781312	-0.048932	4.563692
238.028218	7153.185398	14.786317	-0.048952	4.561243
237.827013	7145.180213	14.791322	-0.048910	4.558770
237.658029	7137.183348	14.796327	-0.048873	4.556298
237.804667	7129.145961	14.801331	-0.048895	4.553813
237.844861	7121.071089	14.806336	-0.048898	4.551314
237.782163	7113.059656	14.811341	-0.048881	4.548834
237.679400	7105.117329	14.816346	-0.048856	4.546373
237.698481	7097.109177	14.821351	-0.048855	4.543891
237.526276	7089.171939	14.826355	-0.048818	4.541430
237.420381	7081.091816	14.831360	-0.048793	4.538922
237.556684	7073.140368	14.836365	-0.048813	4.536454
237.302235	7065.115328	14.841370	-0.048760	4.533961
237.211504	7057.103770	14.846375	-0.048738	4.531471
237.175699	7049.088254	14.851379	-0.048726	4.528978
237.233910	7041.105607	14.856384	-0.048732	4.526495
237.236240	7033.122715	14.861389	-0.048727	4.524010
237.061420	7025.161560	14.866394	-0.048690	4.521529
237.035651	7017.100565	14.871399	-0.048679	4.519017
237.080335	7009.187657	14.876403	-0.048683	4.516550
236.992541	7001.093048	14.881408	-0.048661	4.514024
237.064669	6993.018704	14.886413	-0.048669	4.511504
236.862449	6984.989118	14.891418	-0.048626	4.508995
236.780885	6977.045947	14.896423	-0.048606	4.506513
236.811344	6969.065289	14.901427	-0.048607	4.504017
236.763042	6961.079779	14.906432	-0.048592	4.501519
236.797995	6953.087999	14.911437	-0.048594	4.499017
236.630003	6945.084615	14.916442	-0.048557	4.496510
236.785763	6937.060775	14.921447	-0.048581	4.493996
236.723363	6929.076340	14.926451	-0.048564	4.491492
236.403437	6921.038260	14.931456	-0.048500	4.488969
236.524741	6913.075935	14.936461	-0.048517	4.486470
236.514193	6905.059745	14.941466	-0.048510	4.483952
236.385901	6897.076120	14.946471	-0.048481	4.481442
236.154847	6889.096138	14.951475	-0.048433	4.478932
236.354827	6881.065446	14.956480	-0.048465	4.476406
236.278647	6873.080941	14.961485	-0.048445	4.473892
236.064249	6865.020277	14.966490	-0.048400	4.471353
236.208060	6857.004744	14.971495	-0.048422	4.468827
236.242589	6849.051383	14.976499	-0.048423	4.466319
236.039959	6841.004397	14.981504	-0.048380	4.463779
235.892086	6833.061270	14.986509	-0.048347	4.461271
235.864420	6825.033268	14.991514	-0.048337	4.458735
235.899584	6817.040671	14.996519	-0.048338	4.456209
235.968201	6809.064021	15.001523	-0.048346	4.453687
235.858122	6800.981715	15.006528	-0.048320	4.451129
235.839549	6793.020227	15.011533	-0.048312	4.448608
235.612934	6785.006899	15.016538	-0.048264	4.446069
235.635556	6777.012631	15.021543	-0.048263	4.443535
235.687932	6769.050073	15.026547	-0.048268	4.441010
235.533083	6761.004402	15.031552	-0.048234	4.438456
235.565778	6753.013889	15.036557	-0.048235	4.435919
235.425338	6744.997977	15.041562	-0.048203	4.433372
235.449273	6736.935281	15.046567	-0.048203	4.430809
235.041125	6728.975783	15.051571	-0.048121	4.428276
235.167524	6720.934662	15.056576	-0.048140	4.425717
235.239037	6712.976403	15.061581	-0.048148	4.423183
235.132421	6705.004809	15.066586	-0.048123	4.420643
235.130943	6696.987284	15.071591	-0.048117	4.418087
235.236269	6689.008952	15.076595	-0.048132	4.415542
235.017975	6680.961065	15.081600	-0.048086	4.412973
234.961671	6672.978907	15.086605	-0.048070	4.410423
235.069078	6664.989966	15.091610	-0.048085	4.407871
235.002028	6656.934273	15.096615	-0.048068	4.405295
234.885388	6648.997315	15.101619	-0.048041	4.402755
234.786167	6640.956471	15.106624	-0.048017	4.400181
234.818978	6633.030214	15.111629	-0.048018	4.397642
234.644350	6624.999099	15.116634	-0.047980	4.395068
234.708966	6616.997835	15.121639	-0.047987	4.392502
234.800170	6608.959908	15.126643	-0.047999	4.389924
234.373308	6600.972767	15.131648	-0.047914	4.387357
234.346858	6592.994016	15.136653	-0.047904	4.384794
234.406534	6584.989264	15.141658	-0.047910	4.382222
234.315682	6576.967680	15.146663	-0.047888	4.379641
234.286847	6569.056413	15.151667	-0.047877	4.377095
234.091974	6560.993892	15.156672	-0.047836	4.374498
234.240436	6552.996626	15.161677	-0.047858	4.371922
234.148532	6544.931140	15.166682	-0.047836	4.369322
234.170485	6536.993132	15.171687	-0.047835	4.366761
234.195377	6528.993964	15.176691	-0.047834	4.364180
233.863976	6521.038402	15.181696	-0.047768	4.361609
233.921214	6513.019130	15.186701	-0.047773	4.359018
233.862252	6505.062920	15.191706	-0.047757	4.356445
233.719274	6496.933700	15.196711	-0.047725	4.353814
233.905405	6488.877956	15.201715	-0.047754	4.351207
233.785246	6480.861215	15.206720	-0.047727	4.348610
233.638844	6472.969275	15.211725	-0.047695	4.346051
233.464026	6464.977741	15.216730	-0.047657	4.343458
233.416237	6456.972982	15.221735	-0.047643	4.340860
233.682381	6449.013443	15.226739	-0.047687	4.338278
233.389407	6440.969714	15.231744	-0.047627	4.335663
233.363804	6432.951076	15.236749	-0.047617	4.333056
233.545328	6424.931783	15.241754	-0.047646	4.330448
233.451426	6416.965539	15.246759	-0.047623	4.327855
233.489685	6408.949415	15.251763	-0.047625	4.325245
233.303070	6400.982452	15.256768	-0.047585	4.322647
233.309216	6392.987270	15.261773	-0.047581	4.320040
233.046308	6385.021253	15.266778	-0.047527	4.317439
232.983511	6376.933158	15.271783	-0.047510	4.314799
233.012942	6368.924337	15.276787	-0.047511	4.312183
232.958075	6360.898479	15.281792	-0.047495	4.309559
233.094007	6352.948412	15.286797	-0.047515	4.306960
232.853645	6344.932917	15.291802	-0.047465	4.304335
232.869645	6336.959140	15.296807	-0.047463	4.301724
232.795187	6328.939057	15.301811	-0.047444	4.299095
232.599348	6320.927835	15.306816	-0.047403	4.296467
232.718023	6312.960471	15.311821	-0.047419	4.293855
232.476062	6304.900382	15.316826	-0.047369	4.291207
232.435118	6296.893554	15.321831	-0.047356	4.288576
232.511864	6288.929529	15.326835	-0.047366	4.285960
232.298905	6280.929305	15.331840	-0.047321	4.283327
232.252111	6272.954498	15.336845	-0.047307	4.280702
232.334162	6264.919676	15.341850	-0.047317	4.278057
232.355917	6256.963356	15.346855	-0.047316	4.275436
232.596472	6248.874597	15.351859	-0.047355	4.272771
232.241315	6240.857596	15.356864	-0.047284	4.270124
232.342027	6232.910192	15.361869	-0.047298	4.267501
232.271519	6224.891904	15.366874	-0.047279	4.264852
232.068085	6216.924713	15.371879	-0.047236	4.262217
232.009372	6208.889716	15.376883	-0.047220	4.259559
231.908188	6200.938265	15.381888	-0.047196	4.256927
231.849675	6192.913315	15.386893	-0.047180	4.254269
231.868995	6184.911976	15.391898	-0.047178	4.251619
231.733889	6176.854044	15.396903	-0.047148	4.248946
231.746039	6168.909998	15.401907	-0.047145	4.246311
231.778364	6160.860311	15.406912	-0.047146	4.243639
231.787439	6152.971387	15.411917	-0.047143	4.241018
231.868054	6144.950070	15.416922	-0.047152	4.238353
231.815586	6136.957325	15.421927	-0.047137	4.235694
231.877258	6128.951302	15.426931	-0.047144	4.233031
231.751811	6120.903294	15.431936	-0.047115	4.230350
231.568854	6112.946440	15.436941	-0.047076	4.227697
231.375825	6104.903227	15.441946	-0.047035	4.225013
231.515355	6096.928248	15.446951	-0.047056	4.222354
231.566677	6088.952481	15.451955	-0.047060	4.219691
231.190098	6081.007755	15.456960	-0.046985	4.217034
231.089330	6072.952430	15.461965	-0.046961	4.214340
231.239544	6064.948734	15.466970	-0.046984	4.211664
231.108330	6056.909324	15.471975	-0.046954	4.208972
231.284248	6048.927096	15.476979	-0.046981	4.206301
231.273245	6040.943603	15.481984	-0.046974	4.203625
231.172410	6032.937313	15.486989	-0.046950	4.200939
231.105904	6024.973242	15.491994	-0.046933	4.198266
231.115417	6016.929133	15.496999	-0.046929	4.195565
231.084909	6008.867337	15.502003	-0.046918	4.192857
230.907211	6000.830361	15.507008	-0.046880	4.190153
230.799830	5992.867811	15.512013	-0.046855	4.187473
230.646280	5984.899860	15.517018	-0.046821	4.184789
230.662657	5976.915773	15.522023	-0.046819	4.182099
230.725638	5968.932508	15.527027	-0.046826	4.179409
230.675322	5960.960898	15.532032	-0.046811	4.176720
230.657130	5952.868542	15.537037	-0.046802	4.173988
230.563567	5944.880133	15.542042	-0.046780	4.171289
230.447607	5936.883843	15.547047	-0.046753	4.168586
230.353520	5928.903129	15.552051	-0.046730	4.165886
230.176532	5920.924929	15.557056	-0.046692	4.163184
230.267057	5912.961243	15.562061	-0.046704	4.160489
230.312448	5904.921347	15.567066	-0.046707	4.157765
230.109203	5896.892574	15.572071	-0.046664	4.155040
230.251869	5888.919641	15.577075	-0.046686	4.152337
230.121716	5880.846511	15.582080	-0.046656	4.149595
230.249873	5872.879906	15.587085	-0.046675	4.146890
230.178251	5864.887900	15.592090	-0.046656	4.144172
230.096551	5856.885936	15.597095	-0.046636	4.141449
230.196222	5848.906610	15.602099	-0.046649	4.138734
230.201678	5840.913893	15.607104	-0.046645	4.136012
230.094444	5832.909468	15.612109	-0.046620	4.133282
229.982521	5824.874865	15.617114	-0.046594	4.130540
229.681805	5816.887316	15.622119	-0.046533	4.127811
229.832092	5808.870296	15.627123	-0.046556	4.125074
229.645475	5800.903890	15.632128	-0.046516	4.122350
229.555157	5792.901834	15.637133	-0.046494	4.119612
229.324144	5784.924997	15.642138	-0.046446	4.116879
229.414081	5776.882250	15.647143	-0.046457	4.114126
229.455317	5768.884039	15.652147	-0.046460	4.111386
229.271308	5760.838727	15.657152	-0.046420	4.108625
229.317449	5752.853787	15.662157	-0.046423	4.105886
229.546226	5744.851704	15.667162	-0.046461	4.103141
229.379949	5736.927350	15.672167	-0.046425	4.100416
229.162238	5728.982193	15.677171	-0.046379	4.097682
229.117258	5720.915968	15.682176	-0.046366	4.094906
228.974968	5712.919783	15.687181	-0.046334	4.092151
229.001115	5704.876222	15.692186	-0.046334	4.089380
228.676215	5696.927127	15.697191	-0.046268	4.086635
228.829915	5688.922884	15.702195	-0.046291	4.083876
228.846602	5680.947545	15.707200	-0.046289	4.081123
228.892395	5672.964676	15.712205	-0.046293	4.078366
228.636727	5664.958718	15.717210	-0.046240	4.075595
228.567907	5656.937217	15.722215	-0.046222	4.072819
228.595097	5648.910101	15.727219	-0.046222	4.070041
228.757706	5640.882923	15.732224	-0.046247	4.067263
228.715144	5632.889408	15.737229	-0.046234	4.064491
228.376881	5624.985556	15.742234	-0.046166	4.061745
228.431047	5616.945943	15.747239	-0.046170	4.058955
228.728517	5608.951123	15.752243	-0.046221	4.056182
228.450176	5600.940860	15.757248	-0.046164	4.053394
228.388669	5592.918142	15.762253	-0.046147	4.050603
228.369607	5584.939542	15.767258	-0.046138	4.047825
228.223983	5576.900123	15.772263	-0.046106	4.045023
228.348552	5568.985554	15.777267	-0.046124	4.042266
228.154080	5560.928043	15.782272	-0.046083	4.039453
228.233735	5552.963695	15.787277	-0.046092	4.036675
228.049503	5544.907194	15.792282	-0.046053	4.033858
227.899292	5536.808496	15.797287	-0.046019	4.031025
227.916749	5528.890279	15.802291	-0.046018	4.028256
227.750184	5520.875889	15.807296	-0.045981	4.025448
227.808014	5512.919670	15.812301	-0.045987	4.022662
227.869768	5504.912675	15.817306	-0.045993	4.019857
227.531750	5496.953906	15.822311	-0.045925	4.017060
227.465393	5488.924698	15.827315	-0.045908	4.014241
227.579159	5480.877997	15.832320	-0.045924	4.011417
227.586581	5472.907411	15.837325	-0.045920	4.008615
227.264424	5464.915578	15.842330	-0.045855	4.005799
227.100114	5456.893089	15.847335	-0.045819	4.002973
227.220100	5448.925420	15.852339	-0.045836	4.000168
227.419130	5440.926919	15.857344	-0.045868	3.997352
227.098202	5432.950779	15.862349	-0.045803	3.994534
227.206117	5424.898740	15.867354	-0.045818	3.991693
227.276326	5416.878880	15.872359	-0.045826	3.988862
227.072926	5408.917148	15.877363	-0.045783	3.986044
226.861341	5400.890937	15.882368	-0.045738	3.983202
226.979390	5392.907993	15.887373	-0.045755	3.980378
226.990982	5384.973569	15.892378	-0.045752	3.977567
227.052831	5376.924405	15.897383	-0.045758	3.974715
226.936149	5368.939622	15.902387	-0.045731	3.971881
226.685928	5360.911574	15.907392	-0.045680	3.969026
226.712640	5352.961374	15.912397	-0.045679	3.966203
226.877564	5344.939083	15.917402	-0.045705	3.963353
226.941691	5336.965082	15.922407	-0.045712	3.960518
226.777084	5329.020124	15.927411	-0.045676	3.957686
226.659421	5320.978783	15.932416	-0.045649	3.954819
226.848714	5312.947600	15.937421	-0.045679	3.951959
226.561727	5304.952503	15.942426	-0.045620	3.949102
226.365960	5296.957957	15.947431	-0.045579	3.946244
226.459691	5288.954116	15.952435	-0.045591	3.943386
226.404769	5280.988730	15.957440	-0.045576	3.940537
226.299341	5273.007229	15.962445	-0.045551	3.937679
226.377738	5264.983166	15.967450	-0.045560	3.934807
226.269226	5256.962121	15.972455	-0.045535	3.931930
226.157164	5248.989820	15.977459	-0.045509	3.929069
225.904790	5240.993082	15.982464	-0.045457	3.926195
225.963134	5233.002184	15.987469	-0.045462	3.923326
225.964287	5225.011343	15.992474	-0.045457	3.920454
225.863032	5217.020321	15.997479	-0.045433	3.917578
225.870652	5209.030495	16.002483	-0.045429	3.914703
225.749571	5201.015053	16.007488	-0.045402	3.911813
225.657297	5192.972934	16.012493	-0.045379	3.908913
225.558523	5184.969178	16.017498	-0.045356	3.906023
225.488279	5176.994976	16.022503	-0.045338	3.903143
225.389182	5169.038572	16.027507	-0.045314	3.900267
225.337578	5161.000998	16.032512	-0.045299	3.897360
225.320455	5152.977120	16.037517	-0.045291	3.894457
225.356030	5145.002135	16.042522	-0.045292	3.891570
225.256138	5136.958430	16.047527	-0.045268	3.888653
225.321005	5128.982602	16.052531	-0.045275	3.885762
225.300352	5121.001781	16.057536	-0.045266	3.882866
225.120583	5113.017425	16.062541	-0.045228	3.879963
224.957157	5105.049410	16.067546	-0.045192	3.877063
224.968434	5096.965586	16.072551	-0.045189	3.874123
225.072854	5088.759384	16.077555	-0.045203	3.871138
224.848527	5080.833532	16.082560	-0.045156	3.868247
224.948933	5072.868572	16.087565	-0.045170	3.865345
224.997419	5064.939778	16.092570	-0.045174	3.862454
224.960407	5056.954936	16.097575	-0.045161	3.859538
225.069072	5049.003129	16.102579	-0.045177	3.856635
224.796444	5040.992190	16.107584	-0.045121	3.853700
224.585743	5033.013031	16.112589	-0.045076	3.850776
224.773647	5024.981999	16.117594	-0.045106	3.847839
224.671702	5016.978361	16.122599	-0.045082	3.844903
224.784059	5009.049683	16.127603	-0.045098	3.841998
224.412959	5001.036878	16.132608	-0.045023	3.839049
224.490368	4993.078092	16.137613	-0.045033	3.836127
224.235910	4985.070320	16.142618	-0.044980	3.833178
224.155781	4977.016485	16.147623	-0.044960	3.830213
224.107088	4969.067998	16.152627	-0.044946	3.827286
224.232177	4960.997079	16.157632	-0.044964	3.824315
224.112246	4953.109820	16.162637	-0.044936	3.821404
224.171985	4945.087179	16.167642	-0.044942	3.818444
224.056615	4937.079190	16.172647	-0.044916	3.815484
224.128093	4929.078435	16.177651	-0.044924	3.812529
223.733258	4921.042709	16.182656	-0.044845	3.809548
223.864599	4913.079618	16.187661	-0.044864	3.806603
223.822062	4905.115996	16.192666	-0.044851	3.803652
223.753777	4897.128953	16.197671	-0.044833	3.800689
223.744917	4889.124477	16.202675	-0.044826	3.797719
223.811763	4881.077245	16.207680	-0.044834	3.794732
223.601541	4873.058681	16.212685	-0.044789	3.791747
223.480047	4865.071442	16.217690	-0.044762	3.788774
223.446789	4857.061775	16.222695	-0.044750	3.785792
223.502356	4849.085778	16.227699	-0.044755	3.782822
223.440862	4841.074529	16.232704	-0.044739	3.779834
223.405312	4833.105718	16.237709	-0.044727	3.776860
223.542626	4825.120190	16.242714	-0.044747	3.773881
223.388703	4817.049227	16.247719	-0.044713	3.770861
223.394932	4809.090184	16.252723	-0.044709	3.767885
223.185808	4801.072239	16.257728	-0.044665	3.764879
223.126829	4793.143218	16.262733	-0.044649	3.761907
222.994268	4785.129295	16.267738	-0.044619	3.758900
222.992343	4777.097143	16.272743	-0.044614	3.755886
223.112268	4769.124563	16.277747	-0.044631	3.752895
222.978369	4761.066117	16.282752	-0.044601	3.749864
222.874205	4753.082928	16.287757	-0.044576	3.746859
222.919776	4745.110921	16.292762	-0.044580	3.743859
222.644887	4737.117352	16.297767	-0.044523	3.740842
222.772715	4729.154674	16.302771	-0.044542	3.737843
222.776062	4721.135895	16.307776	-0.044537	3.734817
222.576709	4713.148026	16.312781	-0.044495	3.731796
222.438236	4705.131474	16.317786	-0.044464	3.728763
222.624886	4697.122245	16.322791	-0.044494	3.725738
222.658679	4689.169611	16.327795	-0.044495	3.722728
222.322975	4681.193544	16.332800	-0.044427	3.719699
222.230727	4673.248805	16.337805	-0.044405	3.716684
222.487145	4665.178694	16.342810	-0.044447	3.713628
222.091349	4657.088288	16.347815	-0.044368	3.710545
222.315137	4649.134536	16.352819	-0.044405	3.707528
222.105072	4641.138288	16.357824	-0.044360	3.704481
222.323944	4633.166623	16.362829	-0.044396	3.701451
222.092666	4625.190730	16.367834	-0.044348	3.698406
221.756217	4617.210417	16.372839	-0.044280	3.695354
221.917255	4609.220444	16.377843	-0.044305	3.692309
221.785728	4601.172989	16.382848	-0.044275	3.689232
221.624201	4593.231438	16.387853	-0.044240	3.686191
221.742729	4585.238763	16.392858	-0.044257	3.683136
221.568494	4577.222468	16.397863	-0.044219	3.680062
221.597728	4569.300326	16.402867	-0.044219	3.677026
221.535773	4561.248455	16.407872	-0.044203	3.673936
221.707215	4553.182829	16.412877	-0.044229	3.670844
221.660946	4545.237690	16.417882	-0.044216	3.667790
221.564191	4537.210906	16.422887	-0.044192	3.664701
221.651949	4529.266813	16.427891	-0.044204	3.661646
221.299380	4521.288764	16.432896	-0.044133	3.658563
221.129054	4513.278467	16.437901	-0.044096	3.655471
221.190811	4505.233284	16.442906	-0.044102	3.652368
221.175461	4497.219595	16.447911	-0.044094	3.649273
221.035035	4489.281872	16.452915	-0.044063	3.646201
220.997624	4481.268780	16.457920	-0.044051	3.643101
220.894426	4473.293679	16.462925	-0.044026	3.640010
221.022164	4465.311808	16.467930	-0.044045	3.636921
220.840659	4457.292187	16.472935	-0.044006	3.633805
220.932434	4449.248419	16.477939	-0.044018	3.630686
220.855682	4441.224917	16.482944	-0.043998	3.627566
220.921172	4433.243329	16.487949	-0.044005	3.624465
220.918625	4425.314229	16.492954	-0.044000	3.621379
220.596917	4417.306230	16.497959	-0.043935	3.618251
220.825771	4409.327228	16.502963	-0.043972	3.615147
220.516165	4401.312366	16.507968	-0.043909	3.612011
220.457175	4393.311570	16.512973	-0.043893	3.608885
220.506611	4385.328375	16.517978	-0.043897	3.605766
220.253799	4377.352130	16.522983	-0.043845	3.602639
220.336381	4369.389983	16.527987	-0.043855	3.599524
220.281691	4361.418280	16.532992	-0.043840	3.596398
220.053943	4353.376892	16.537997	-0.043792	3.593238
220.277318	4345.338720	16.543002	-0.043829	3.590089
220.371385	4337.343875	16.548007	-0.043841	3.586950
220.153422	4329.381030	16.553011	-0.043795	3.583812
220.059492	4321.400375	16.558016	-0.043772	3.580669
220.251265	4313.409088	16.563021	-0.043803	3.577526
220.091430	4305.395868	16.568026	-0.043768	3.574362
219.789620	4297.391543	16.573031	-0.043707	3.571194
219.984549	4289.419533	16.578035	-0.043738	3.568051
219.884458	4281.424923	16.583040	-0.043714	3.564887
219.795408	4273.442165	16.588045	-0.043692	3.561726
219.621448	4265.437380	16.593050	-0.043655	3.558551
219.687408	4257.433793	16.598055	-0.043662	3.555380
219.777740	4249.360785	16.603059	-0.043673	3.552180
219.424092	4241.354134	16.608064	-0.043602	3.548990
219.375883	4233.386916	16.613069	-0.043588	3.545821
219.563618	4225.419316	16.618074	-0.043618	3.542657
219.401187	4217.398924	16.623079	-0.043583	3.539459
219.255121	4209.463708	16.628083	-0.043550	3.536292
219.373598	4201.425680	16.633088	-0.043567	3.533089
219.242979	4193.410673	16.638093	-0.043538	3.529885
219.184893	4185.443560	16.643098	-0.043522	3.526699
219.096844	4177.421991	16.648103	-0.043500	3.523488
219.237309	4169.493968	16.653107	-0.043521	3.520318
219.081259	4161.506987	16.658112	-0.043487	3.517113
219.136339	4153.483125	16.663117	-0.043492	3.513896
219.088013	4145.474559	16.668122	-0.043478	3.510680
218.766447	4137.471173	16.673127	-0.043413	3.507454
218.789810	4129.504450	16.678131	-0.043412	3.504250
218.748515	4121.530648	16.683136	-0.043399	3.501039
218.619794	4113.542336	16.688141	-0.043370	3.497816
218.618889	4105.563083	16.693146	-0.043364	3.494598
218.501509	4097.553143	16.698151	-0.043337	3.491361
218.595610	4089.563455	16.703155	-0.043350	3.488135
218.390389	4081.575328	16.708160	-0.043306	3.484898
218.382395	4073.623120	16.713165	-0.043300	3.481679
218.407738	4065.614802	16.718170	-0.043299	3.478435
218.497041	4057.603496	16.723175	-0.043311	3.475188
218.203437	4049.590064	16.728179	-0.043251	3.471926
218.248560	4041.566566	16.733184	-0.043254	3.468667
218.092845	4033.581191	16.738189	-0.043220	3.465414
218.034865	4025.606306	16.743194	-0.043204	3.462166
217.889260	4017.621456	16.748199	-0.043172	3.458907
218.054122	4009.616961	16.753203	-0.043197	3.455648
217.772713	4001.622259	16.758208	-0.043140	3.452375
217.804860	3993.586286	16.763213	-0.043140	3.449092
217.893431	3985.649514	16.768218	-0.043152	3.445849
217.552015	3977.673505	16.773223	-0.043083	3.442572
217.612454	3969.668009	16.778227	-0.043089	3.439293
217.531349	3961.698396	16.783232	-0.043069	3.436021
217.577528	3953.650018	16.788237	-0.043072	3.432718
217.474377	3945.654248	16.793242	-0.043048	3.429428
217.462017	3937.669369	16.798247	-0.043040	3.426143
217.598271	3929.664775	16.803251	-0.043060	3.422852
217.518521	3921.704564	16.808256	-0.043040	3.419568
217.289185	3913.734910	16.813261	-0.042993	3.416272
217.296085	3905.741393	16.818266	-0.042989	3.412971
217.305115	3897.670889	16.823271	-0.042985	3.409635
217.199941	3889.758814	16.828275	-0.042960	3.406358
216.987744	3881.765394	16.833280	-0.042916	3.403040
217.082698	3873.748917	16.838285	-0.042928	3.399719
217.158947	3865.822257	16.843290	-0.042937	3.396433
217.077861	3857.742179	16.848295	-0.042917	3.393073
216.914300	3849.715365	16.853299	-0.042881	3.389730
216.739592	3841.752222	16.858304	-0.042844	3.386409
216.665765	3833.761477	16.863309	-0.042825	3.383078
216.659517	3825.811822	16.868314	-0.042818	3.379762
216.539124	3817.824361	16.873319	-0.042791	3.376423
216.559457	3809.814206	16.878323	-0.042789	3.373077
216.728009	3801.773230	16.883328	-0.042816	3.369720
216.798361	3793.817161	16.888333	-0.042824	3.366391
216.731388	3785.847950	16.893338	-0.042806	3.363048
216.514975	3777.850452	16.898343	-0.042760	3.359685
216.508588	3769.921738	16.903347	-0.042754	3.356355
216.499562	3761.882360	16.908352	-0.042747	3.352976
216.309033	3753.877184	16.913357	-0.042707	3.349600
216.340609	3745.888319	16.918362	-0.042707	3.346236
216.103128	3737.887941	16.923367	-0.042658	3.342854
216.295719	3729.887884	16.928371	-0.042689	3.339485
216.216100	3721.942474	16.933376	-0.042669	3.336125
216.131136	3713.934012	16.938381	-0.042648	3.332734
215.996112	3705.931499	16.943386	-0.042617	3.329341
215.814509	3697.954559	16.948391	-0.042578	3.325954
215.959829	3689.971753	16.953395	-0.042600	3.322573
215.771080	3681.963305	16.958400	-0.042560	3.319165
215.621181	3674.026535	16.963405	-0.042527	3.315785
215.820021	3665.988554	16.968410	-0.042559	3.312372
215.548066	3657.953715	16.973415	-0.042503	3.308939
215.474156	3650.009234	16.978419	-0.042484	3.305549
215.404454	3642.033824	16.983424	-0.042466	3.302142
215.331640	3634.023146	16.988429	-0.042447	3.298716
215.384862	3626.051113	16.993434	-0.042452	3.295308
215.247313	3618.047600	16.998439	-0.042421	3.291876
215.397005	3610.036112	17.003443	-0.042444	3.288448
215.203227	3602.064621	17.008448	-0.042402	3.285020
215.033356	3594.119000	17.013453	-0.042366	3.281600
215.086841	3586.112892	17.018458	-0.042370	3.278160
215.023125	3578.104059	17.023463	-0.042353	3.274710
214.884571	3570.129337	17.028467	-0.042322	3.271268
214.840571	3562.097309	17.033472	-0.042309	3.267802
214.935598	3554.086419	17.038477	-0.042321	3.264346
214.808618	3546.180813	17.043482	-0.042293	3.260924
214.573753	3538.144202	17.048487	-0.042244	3.257437
214.662106	3530.146383	17.053491	-0.042255	3.253976
214.640672	3522.134050	17.058496	-0.042246	3.250501
214.723466	3514.163804	17.063501	-0.042256	3.247044
214.740623	3506.188696	17.068506	-0.042254	3.243579
214.688324	3498.192682	17.073511	-0.042239	3.240098
214.737464	3490.241720	17.078515	-0.042243	3.236637
214.591819	3482.215746	17.083520	-0.042211	3.233132
214.500196	3474.178496	17.088525	-0.042189	3.229621
214.386185	3466.242826	17.093530	-0.042162	3.226149
214.127774	3458.234407	17.098535	-0.042109	3.222635
214.192805	3450.249382	17.103539	-0.042116	3.219141
214.137085	3442.272254	17.108544	-0.042100	3.215642
214.113018	3434.263884	17.113549	-0.042091	3.212127
214.040395	3426.303684	17.118554	-0.042072	3.208627
213.986741	3418.286560	17.123559	-0.042057	3.205099
214.007346	3410.340703	17.128563	-0.042055	3.201601
213.992418	3402.355929	17.133568	-0.042048	3.198081
213.876287	3394.359894	17.138573	-0.042021	3.194548
213.817191	3386.363085	17.143578	-0.042005	3.191013
213.772916	3378.357526	17.148583	-0.041991	3.187470
213.685060	3370.400304	17.153587	-0.041970	3.183944
213.753439	3362.379219	17.158592	-0.041977	3.180392
213.443768	3354.442810	17.163597	-0.041914	3.176857
213.386651	3346.438365	17.168602	-0.041899	3.173299
213.521864	3338.394185	17.173607	-0.041918	3.169727
213.513426	3330.441592	17.178611	-0.041912	3.166186
213.264829	3322.495986	17.183616	-0.041860	3.162634
213.294736	3314.486224	17.188621	-0.041861	3.159061
213.388377	3306.507944	17.193626	-0.041873	3.155501
213.097960	3298.486086	17.198631	-0.041814	3.151901
212.939383	3290.494802	17.203635	-0.041779	3.148316
212.955233	3282.481700	17.208640	-0.041777	3.144725
212.906657	3274.525785	17.213645	-0.041763	3.141152
213.124346	3266.536797	17.218650	-0.041798	3.137572
212.997604	3258.551903	17.223655	-0.041769	3.133975
212.916758	3250.549540	17.228659	-0.041749	3.130368
212.804193	3242.585880	17.233664	-0.041723	3.126773
212.846537	3234.604337	17.238669	-0.041726	3.123172
212.867087	3226.629311	17.243674	-0.041724	3.119569
212.625794	3218.670224	17.248679	-0.041674	3.115958
212.577741	3210.666095	17.253683	-0.041660	3.112330
212.683544	3202.641511	17.258688	-0.041674	3.108696
212.459393	3194.635218	17.263693	-0.041628	3.105051
212.473226	3186.715496	17.268698	-0.041625	3.101452
212.212584	3178.719394	17.273703	-0.041571	3.097802
212.437660	3170.719586	17.278707	-0.041608	3.094168
212.131214	3162.729984	17.283712	-0.041546	3.090509
212.066330	3154.744045	17.288717	-0.041528	3.086859
212.208677	3146.765039	17.293722	-0.041550	3.083218
212.038503	3138.771187	17.298727	-0.041513	3.079551
212.063157	3130.839998	17.303731	-0.041512	3.075917
211.984032	3122.749895	17.308736	-0.041492	3.072201
211.843958	3114.726776	17.313741	-0.041461	3.068509
211.992084	3106.747027	17.318746	-0.041484	3.064845
211.689728	3098.812698	17.323751	-0.041422	3.061177
211.738774	3090.858762	17.328755	-0.041426	3.057512
211.625808	3082.871507	17.333760	-0.041400	3.053820
211.571949	3074.856833	17.338765	-0.041385	3.050113
211.431099	3066.909451	17.343770	-0.041353	3.046429
211.281222	3058.928915	17.348775	-0.041320	3.042724
211.343008	3050.965188	17.353779	-0.041327	3.039033
211.430523	3042.978206	17.358784	-0.041338	3.035328
211.237406	3034.960312	17.363789	-0.041297	3.031590
211.329428	3026.958242	17.368794	-0.041309	3.027869
211.110149	3018.978351	17.373799	-0.041263	3.024139
211.274739	3010.999061	17.378803	-0.041288	3.020423
211.116354	3003.046627	17.383808	-0.041253	3.016699
211.033696	2995.034137	17.388813	-0.041233	3.012946
211.201031	2987.022725	17.393818	-0.041259	3.009201
210.979251	2979.072802	17.398823	-0.041212	3.005461
210.915614	2971.112228	17.403827	-0.041195	3.001719
210.886190	2963.137430	17.408832	-0.041185	2.997968
210.663200	2955.151369	17.413837	-0.041138	2.994197
210.556763	2947.147243	17.418842	-0.041113	2.990418
210.369103	2939.153326	17.423847	-0.041073	2.986636
210.472470	2931.176954	17.428851	-0.041087	2.982871
210.458185	2923.188197	17.433856	-0.041079	2.979090
210.295219	2915.223496	17.438861	-0.041044	2.975308
210.296045	2907.225176	17.443866	-0.041039	2.971514
210.010929	2899.234228	17.448871	-0.040980	2.967703
210.107768	2891.248098	17.453875	-0.040993	2.963910
210.270879	2883.272220	17.458880	-0.041018	2.960120
210.204373	2875.319442	17.463885	-0.041001	2.956324
210.150783	2867.325204	17.468890	-0.040986	2.952504
210.196155	2859.301924	17.473895	-0.040989	2.948671
210.076988	2851.327086	17.478899	-0.040962	2.944847
209.796270	2843.397128	17.483904	-0.040904	2.941031
209.696405	2835.424143	17.488909	-0.040880	2.937199
209.863493	2827.412413	17.493914	-0.040906	2.933358
209.958373	2819.357378	17.498919	-0.040919	2.929486
209.691668	2811.447000	17.503923	-0.040864	2.925661
209.353282	2803.496116	17.508928	-0.040796	2.921806
209.386282	2795.508058	17.513933	-0.040797	2.917949
209.291099	2787.533670	17.518938	-0.040774	2.914086
209.073656	2779.451981	17.523943	-0.040728	2.910159
209.309306	2771.462555	17.528947	-0.040767	2.906297
209.283794	2763.518903	17.533952	-0.040757	2.902437
209.116448	2755.536738	17.538957	-0.040721	2.898546
209.250366	2747.567218	17.543962	-0.040740	2.894672
208.953141	2739.589002	17.548967	-0.040680	2.890765
208.910533	2731.623433	17.553971	-0.040667	2.886872
209.190803	2723.624993	17.558976	-0.040714	2.882977
208.985221	2715.669151	17.563981	-0.040670	2.879070
208.799167	2707.725216	17.568986	-0.040631	2.875164
208.712912	2699.707287	17.573991	-0.040609	2.871223
208.669855	2691.720314	17.578995	-0.040596	2.867293
208.630487	2683.753403	17.584000	-0.040584	2.863369
208.432567	2675.760236	17.589005	-0.040542	2.859417
208.574606	2667.816977	17.594010	-0.040563	2.855503
208.442813	2659.789258	17.599015	-0.040533	2.851527
208.343937	2651.825798	17.604019	-0.040510	2.847579
208.146558	2643.876422	17.609024	-0.040468	2.843627
208.245204	2635.860599	17.614029	-0.040481	2.839653
208.256530	2627.919843	17.619034	-0.040478	2.835706
208.122188	2619.902084	17.624039	-0.040448	2.831706
208.382661	2611.890084	17.629043	-0.040491	2.827727
208.345164	2603.912665	17.634048	-0.040479	2.823742
208.091747	2595.970631	17.639053	-0.040427	2.819757
208.003428	2588.029747	17.644058	-0.040405	2.815776
207.850978	2580.021020	17.649063	-0.040371	2.811751
207.783063	2572.055120	17.654067	-0.040354	2.807748
207.780168	2564.075749	17.659072	-0.040348	2.803735
207.828564	2556.078955	17.664077	-0.040352	2.799711
207.667265	2548.154388	17.669082	-0.040317	2.795706
207.479378	2540.150446	17.674087	-0.040276	2.791653
207.694130	2532.150978	17.679091	-0.040311	2.787620
207.513449	2524.172596	17.684096	-0.040272	2.783568
207.330536	2516.203114	17.689101	-0.040233	2.779516
207.410034	2508.268795	17.694106	-0.040243	2.775490
207.436881	2500.234956	17.699111	-0.040243	2.771405
207.384069	2492.273097	17.704115	-0.040228	2.767346
207.091626	2484.324743	17.709120	-0.040168	2.763273
207.082036	2476.364217	17.714125	-0.040161	2.759205
207.159386	2468.392407	17.719130	-0.040170	2.755130
206.879282	2460.332004	17.724135	-0.040113	2.750983
206.911014	2452.335862	17.729139	-0.040114	2.746881
207.073331	2444.365951	17.734144	-0.040139	2.742794
206.527924	2436.452821	17.739149	-0.040032	2.738688
206.556480	2428.492279	17.744154	-0.040032	2.734585
206.575235	2420.449971	17.749159	-0.040030	2.730434
206.711355	2412.472279	17.754163	-0.040051	2.726317
206.613786	2404.531994	17.759168	-0.040027	2.722199
206.503708	2396.569184	17.764173	-0.040002	2.718062
206.582544	2388.603181	17.769178	-0.040011	2.713928
206.256106	2380.618041	17.774183	-0.039945	2.709754
206.266609	2372.654076	17.779187	-0.039942	2.705605
206.171781	2364.686877	17.784192	-0.039919	2.701441
206.090293	2356.714293	17.789197	-0.039899	2.697269
206.156874	2348.727903	17.794202	-0.039906	2.693092
206.101018	2340.715091	17.799207	-0.039891	2.688887
206.105148	2332.771749	17.804211	-0.039886	2.684716
205.942007	2324.827190	17.809216	-0.039851	2.680527
205.824720	2316.872997	17.814221	-0.039824	2.676330
205.863801	2308.857959	17.819226	-0.039826	2.672104
205.686197	2300.872492	17.824231	-0.039787	2.667872
205.521395	2292.915915	17.829235	-0.039752	2.663650
205.719171	2284.923676	17.834240	-0.039783	2.659426
205.674727	2276.958937	17.839245	-0.039770	2.655195
205.646660	2268.985556	17.844250	-0.039759	2.650952
205.432678	2261.000605	17.849255	-0.039714	2.646685
205.441116	2253.050451	17.854259	-0.039711	2.642444
205.255226	2245.111855	17.859264	-0.039671	2.638189
205.203786	2237.120941	17.864269	-0.039656	2.633909
205.201931	2229.143909	17.869274	-0.039651	2.629632
205.073540	2221.184742	17.874279	-0.039622	2.625349
205.190565	2213.191150	17.879283	-0.039638	2.621058
205.361128	2205.215810	17.884288	-0.039665	2.616772
204.941608	2197.271491	17.889293	-0.039582	2.612457
204.909510	2189.297271	17.894298	-0.039571	2.608144
204.916688	2181.306589	17.899303	-0.039567	2.603818
204.843714	2173.345504	17.904307	-0.039548	2.599496
204.798936	2165.415997	17.909312	-0.039535	2.595185
204.682576	2157.253263	17.914317	-0.039508	2.590735
204.769437	2149.292317	17.919322	-0.039519	2.586402
204.570979	2141.363043	17.924327	-0.039476	2.582059
204.521132	2133.452212	17.929331	-0.039462	2.577729
204.558397	2125.480814	17.934336	-0.039464	2.573364
204.547969	2117.490275	17.939341	-0.039457	2.568978
204.473913	2109.542413	17.944346	-0.039438	2.564604
204.411403	2101.589412	17.949351	-0.039421	2.560220
204.424485	2093.641056	17.954355	-0.039418	2.555837
204.225899	2085.680957	17.959360	-0.039376	2.551425
203.990962	2077.717382	17.964365	-0.039327	2.547000
204.191994	2069.738186	17.969370	-0.039360	2.542590
204.050439	2061.790251	17.974375	-0.039328	2.538165
203.966321	2053.835471	17.979379	-0.039307	2.533733
203.902472	2045.830787	17.984384	-0.039290	2.529267
203.697180	2037.885474	17.989389	-0.039247	2.524816
203.561148	2029.957682	17.994394	-0.039216	2.520371
203.543579	2021.978919	17.999399	-0.039208	2.515899
203.724814	2013.956002	18.004403	-0.039236	2.511408
203.452993	2006.006494	18.009408	-0.039181	2.506918
203.251882	1998.060332	18.014413	-0.039138	2.502427
203.358045	1990.101299	18.019418	-0.039153	2.497943
203.337725	1982.126508	18.024423	-0.039144	2.493432
203.093548	1974.156883	18.029427	-0.039093	2.488900
203.283693	1966.166730	18.034432	-0.039123	2.484380
203.217485	1958.226224	18.039437	-0.039106	2.479861
203.227865	1950.301214	18.044442	-0.039103	2.475348
202.991525	1942.319205	18.049447	-0.039053	2.470776
202.864114	1934.375816	18.054451	-0.039025	2.466225
203.036620	1926.388080	18.059456	-0.039052	2.461664
202.745159	1918.451033	18.064461	-0.038992	2.457088
202.897293	1910.464014	18.069466	-0.039015	2.452508
202.710507	1902.489458	18.074471	-0.038975	2.447901
202.711146	1894.540789	18.079475	-0.038970	2.443315
202.664440	1886.608415	18.084480	-0.038956	2.438725
202.537509	1878.647451	18.089485	-0.038928	2.434105
202.377971	1870.612727	18.094490	-0.038893	2.429430
202.292494	1862.642241	18.099495	-0.038872	2.424789
202.331948	1854.692734	18.104499	-0.038874	2.420162
202.404277	1846.744419	18.109504	-0.038882	2.415528
202.102225	1838.783421	18.114509	-0.038821	2.410850
202.285295	1830.823573	18.119514	-0.038850	2.406200
202.155340	1822.884818	18.124519	-0.038820	2.401530
202.063766	1814.945856	18.129523	-0.038798	2.396853
202.188403	1806.962860	18.134528	-0.038816	2.392158
201.974618	1799.004012	18.139533	-0.038771	2.387441
202.013159	1791.057263	18.144538	-0.038773	2.382743
201.717466	1783.131804	18.149543	-0.038713	2.378021
201.784801	1775.158268	18.154547	-0.038721	2.373290
201.658474	1767.204364	18.159552	-0.038692	2.368545
201.526647	1759.235312	18.164557	-0.038662	2.363782
201.539578	1751.292614	18.169562	-0.038659	2.359036
201.447772	1743.341231	18.174567	-0.038637	2.354267
201.382013	1735.343491	18.179571	-0.038620	2.349463
201.249608	1727.408520	18.184576	-0.038590	2.344681
201.256615	1719.433106	18.189581	-0.038586	2.339877
201.214230	1711.515898	18.194586	-0.038573	2.335093
201.139712	1703.524447	18.199591	-0.038554	2.330252
201.123966	1695.571212	18.204595	-0.038546	2.325430
201.046649	1687.645702	18.209600	-0.038526	2.320608
200.639891	1679.734338	18.214605	-0.038446	2.315758
200.927930	1671.713279	18.219610	-0.038494	2.310889
200.905142	1663.754836	18.224615	-0.038485	2.306022
200.735636	1655.821117	18.229619	-0.038448	2.301147
200.630792	1647.893393	18.234624	-0.038423	2.296271
200.513234	1639.919433	18.239629	-0.038396	2.291355
200.444211	1631.985806	18.244634	-0.038378	2.286458
200.115841	1624.058823	18.249639	-0.038312	2.281532
200.426365	1616.076990	18.254643	-0.038365	2.276616
200.446556	1608.080993	18.259648	-0.038363	2.271655
200.151594	1600.107501	18.264653	-0.038303	2.266671
200.270927	1592.158032	18.269658	-0.038320	2.261726
200.229788	1584.225688	18.274663	-0.038307	2.256768
200.061493	1576.290132	18.279667	-0.038271	2.251785
199.947368	1568.345808	18.284672	-0.038244	2.246790
199.916029	1560.401462	18.289677	-0.038233	2.241792
199.999286	1552.463529	18.294682	-0.038244	2.236796
199.732251	1544.538955	18.299687	-0.038189	2.231767
199.827904	1536.558689	18.304691	-0.038202	2.226723
199.806115	1528.621748	18.309696	-0.038192	2.221685
199.406966	1520.710722	18.314701	-0.038113	2.216618
199.359752	1512.762417	18.319706	-0.038099	2.211548
199.307451	1504.793053	18.324711	-0.038084	2.206451
199.258013	1496.866310	18.329715	-0.038070	2.201371
199.235720	1488.938748	18.334720	-0.038060	2.196280
199.059881	1480.961859	18.339725	-0.038023	2.191132
198.915202	1473.026975	18.344730	-0.037991	2.186002
198.957164	1465.060933	18.349735	-0.037993	2.180857
198.850139	1457.138897	18.354739	-0.037968	2.175714
198.951009	1449.168630	18.359744	-0.037982	2.170547
198.650478	1441.240655	18.364749	-0.037921	2.165358
198.681102	1433.317864	18.369754	-0.037921	2.160190
198.718032	1425.367328	18.374759	-0.037923	2.154993
198.613766	1417.431629	18.379763	-0.037898	2.149780
198.678283	1409.477312	18.384768	-0.037905	2.144557
198.578951	1401.546870	18.389773	-0.037882	2.139322
198.554055	1393.625443	18.394778	-0.037872	2.134087
198.441529	1385.673421	18.399783	-0.037846	2.128811
198.458966	1377.723407	18.404787	-0.037844	2.123535
198.285629	1369.839829	18.409792	-0.037806	2.118272
197.935101	1361.899873	18.414797	-0.037736	2.112942
197.843197	1353.920439	18.419802	-0.037714	2.107596
197.893225	1345.966331	18.424807	-0.037718	2.102267
197.921911	1338.039832	18.429811	-0.037718	2.096941
197.866246	1330.103103	18.434816	-0.037703	2.091587
197.787029	1322.151610	18.439821	-0.037683	2.086207
197.874068	1314.240894	18.444826	-0.037694	2.080856
197.784001	1306.324363	18.449831	-0.037672	2.075471
197.611480	1298.387340	18.454835	-0.037635	2.070049
197.764508	1290.433030	18.459840	-0.037658	2.064633
197.559142	1282.527729	18.464845	-0.037615	2.059201
197.490470	1274.617270	18.469850	-0.037597	2.053765
197.294998	1266.676834	18.474855	-0.037555	2.048281
197.202521	1258.760065	18.479859	-0.037533	2.042809
197.145949	1250.854545	18.484864	-0.037517	2.037334
197.001761	1242.910166	18.489869	-0.037485	2.031808
197.075488	1234.947970	18.494874	-0.037494	2.026276
196.934486	1227.025495	18.499879	-0.037462	2.020736
196.906517	1219.106569	18.504883	-0.037452	2.015194
196.963793	1211.162581	18.509888	-0.037458	2.009628
196.728115	1203.264657	18.514893	-0.037409	2.004048
196.531388	1195.387308	18.519898	-0.037367	1.998472
196.608799	1187.420384	18.524903	-0.037376	1.992845
196.584004	1179.481625	18.529907	-0.037366	1.987211
196.356470	1171.599949	18.534912	-0.037319	1.981581
196.208449	1163.676527	18.539917	-0.037286	1.975913
196.381679	1155.721423	18.544922	-0.037313	1.970241
196.318326	1147.795972	18.549927	-0.037296	1.964548
196.092791	1139.926895	18.554931	-0.037249	1.958861
196.112606	1131.985725	18.559936	-0.037248	1.953133
195.890808	1124.033435	18.564941	-0.037201	1.947353
195.852238	1116.126754	18.569946	-0.037189	1.941609
195.812015	1108.205613	18.574951	-0.037176	1.935837
195.954906	1100.258311	18.579955	-0.037198	1.930050
195.854964	1092.356010	18.584960	-0.037174	1.924250
195.755879	1084.471087	18.589965	-0.037151	1.918447
195.810848	1076.542571	18.594970	-0.037156	1.912610
195.462116	1068.654395	18.599975	-0.037086	1.906741
195.393437	1060.746207	18.604979	-0.037068	1.900869
195.490782	1052.828679	18.609984	-0.037081	1.894992
195.151593	1044.942625	18.614989	-0.037012	1.889070
195.205614	1037.030456	18.619994	-0.037017	1.883154
195.111154	1029.130195	18.624999	-0.036995	1.877212
195.180007	1021.190758	18.630003	-0.037002	1.871240
195.034225	1013.279038	18.635008	-0.036970	1.865246
194.875266	1005.393213	18.640013	-0.036935	1.859250
195.075341	997.466464	18.645018	-0.036968	1.853245
195.008137	989.552250	18.650023	-0.036950	1.847199
194.860803	981.683191	18.655027	-0.036917	1.841159
194.575625	973.826131	18.660032	-0.036859	1.835091
194.463780	965.915400	18.665037	-0.036833	1.828982
194.301920	958.019915	18.670042	-0.036798	1.822859
194.354886	950.113498	18.675047	-0.036803	1.816732
194.506116	942.171432	18.680051	-0.036826	1.810569
194.354521	934.303667	18.685056	-0.036792	1.804406
194.192245	926.437688	18.690061	-0.036757	1.798222
194.040231	918.536048	18.695066	-0.036724	1.791989
194.042551	910.578594	18.700071	-0.036719	1.785710
194.050935	902.692609	18.705075	-0.036715	1.779466
194.034303	894.813044	18.710080	-0.036707	1.773202
193.739996	886.936762	18.715085	-0.036647	1.766884
193.721366	879.062808	18.720090	-0.036639	1.760579
193.435583	871.225199	18.725095	-0.036580	1.754248
193.453731	863.300154	18.730099	-0.036579	1.747861
193.501894	855.411248	18.735104	-0.036583	1.741484
193.210895	847.559419	18.740109	-0.036523	1.735070
193.292580	839.658663	18.745114	-0.036533	1.728640
193.143973	831.790609	18.750119	-0.036501	1.722184
193.118542	823.921198	18.755123	-0.036491	1.715718
193.006661	816.035699	18.760128	-0.036465	1.709202
193.078270	808.128409	18.765133	-0.036473	1.702668
192.973877	800.277827	18.770138	-0.036449	1.696133
192.623383	792.432753	18.775143	-0.036378	1.689544
192.678418	784.545258	18.780147	-0.036383	1.682948
192.651243	776.691408	18.785152	-0.036373	1.676343
192.617036	768.799621	18.790157	-0.036362	1.669680
192.716809	760.910673	18.795162	-0.036375	1.663009
192.703041	753.051309	18.800167	-0.036367	1.656322
192.420473	745.215735	18.805171	-0.036310	1.649592
192.318351	737.378692	18.810176	-0.036286	1.642857
192.175005	729.530477	18.815181	-0.036254	1.636079
192.280019	721.589064	18.820186	-0.036268	1.629227
192.053641	713.751129	18.825191	-0.036221	1.622389
192.011833	705.897546	18.830195	-0.036208	1.615535
191.789912	698.073961	18.835200	-0.036162	1.608652
191.493763	690.248656	18.840205	-0.036102	1.601728
191.541579	682.402842	18.845210	-0.036105	1.594804
191.424137	674.541555	18.850215	-0.036079	1.587813
191.414289	666.688691	18.855219	-0.036072	1.580814
191.307957	658.868009	18.860224	-0.036047	1.573798
191.119415	651.017218	18.865229	-0.036007	1.566712
191.327416	643.150362	18.870234	-0.036040	1.559637
191.260651	635.312565	18.875239	-0.036023	1.552516
191.150814	627.464221	18.880243	-0.035997	1.545347
191.189366	619.634042	18.885248	-0.035999	1.538182
190.838231	611.841405	18.890253	-0.035929	1.530960
190.934807	603.997697	18.895258	-0.035942	1.523724
190.876893	596.179990	18.900263	-0.035926	1.516454
190.466211	588.401532	18.905267	-0.035844	1.509133
190.420819	580.580166	18.910272	-0.035831	1.501791
190.434825	572.745828	18.915277	-0.035828	1.494409
190.250271	564.942125	18.920282	-0.035789	1.486990
190.164228	557.137147	18.925287	-0.035768	1.479547
189.967112	549.322117	18.930291	-0.035726	1.472040
190.053153	541.460611	18.935296	-0.035737	1.464494
189.910546	533.667329	18.940301	-0.035705	1.456938
189.829412	525.870456	18.945306	-0.035685	1.449350
189.753988	518.070271	18.950311	-0.035666	1.441719
189.654416	510.302031	18.955315	-0.035643	1.434075
189.483777	502.515989	18.960320	-0.035606	1.426361
189.407605	494.720010	18.965325	-0.035587	1.418610
189.581566	486.903851	18.970330	-0.035614	1.410838
189.425776	479.145805	18.975335	-0.035580	1.403027
189.272148	471.387186	18.980339	-0.035546	1.395172
189.182258	463.599792	18.985344	-0.035524	1.387253
188.973910	455.842690	18.990349	-0.035481	1.379300
188.960804	448.070994	18.995354	-0.035473	1.371319
189.015406	440.280993	19.000359	-0.035478	1.363284
188.730268	432.565657	19.005363	-0.035420	1.355220
188.695387	424.799150	19.010368	-0.035409	1.347098
188.564741	417.050025	19.015373	-0.035379	1.338928
188.521016	409.298816	19.020378	-0.035366	1.330721
188.308254	401.579138	19.025383	-0.035322	1.322467
188.185594	393.827674	19.030387	-0.035294	1.314143
188.301667	385.948765	19.035392	-0.035310	1.305671
188.102847	378.254047	19.040397	-0.035268	1.297286
187.956611	370.550621	19.045402	-0.035236	1.288848
187.811009	362.845779	19.050407	-0.035204	1.280352
187.717730	355.143082	19.055411	-0.035182	1.271811
187.580321	347.447658	19.060416	-0.035151	1.263213
187.411340	339.752989	19.065421	-0.035115	1.254550
187.438892	332.038061	19.070426	-0.035115	1.245842
187.336310	324.362302	19.075431	-0.035091	1.237092
187.329195	316.641723	19.080435	-0.035084	1.228246
187.043137	308.998652	19.085440	-0.035026	1.219372
186.830993	301.337957	19.090445	-0.034982	1.210426
186.775384	293.666214	19.095450	-0.034966	1.201432
186.578564	286.025093	19.100455	-0.034925	1.192378
186.470292	278.362130	19.105459	-0.034900	1.183246
186.462890	270.708277	19.110464	-0.034893	1.174075
186.258975	263.069549	19.115469	-0.034850	1.164809
186.237420	255.440002	19.120474	-0.034841	1.155519
185.975605	247.797894	19.125479	-0.034788	1.146087
185.721749	240.202265	19.130483	-0.034735	1.136635
185.848097	232.542562	19.135488	-0.034754	1.127106
185.688244	224.953557	19.140493	-0.034719	1.117523
185.561143	217.363213	19.145498	-0.034691	1.107863
185.224753	209.818909	19.150503	-0.034623	1.098130
185.146307	202.227034	19.155507	-0.034604	1.088306
184.972801	194.683883	19.160512	-0.034567	1.078435
184.770429	187.120598	19.165517	-0.034524	1.068439
184.514489	179.596405	19.170522	-0.034471	1.058389
184.280812	172.066409	19.175527	-0.034423	1.048239
184.050112	164.561318	19.180531	-0.034375	1.038025
183.925918	157.042370	19.185536	-0.034347	1.027715
183.711796	149.546714	19.190541	-0.034303	1.017312
183.383201	142.087976	19.195546	-0.034236	1.006824
182.882977	134.671642	19.200551	-0.034139	0.996244
182.511214	127.192278	19.205555	-0.034064	0.985492
182.167744	119.769625	19.210560	-0.033996	0.974710
181.643982	112.371661	19.215565	-0.033893	0.963798
181.155604	104.995159	19.220570	-0.033798	0.952801
180.724732	97.610928	19.225575	-0.033713	0.941679
180.166636	90.265758	19.230579	-0.033604	0.930450
179.957507	82.885120	19.235584	-0.033560	0.919122
179.167598	75.587663	19.240589	-0.033408	0.907624
178.801826	68.260640	19.245594	-0.033336	0.896048
178.270842	61.189603	19.250599	-0.033232	0.884684