Thu Mar 11 20:20:08 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.705046	0.090375	0.000000	0.000017	0.722075

0.727938	0.089261	0.005005	0.000012	0.722081
0.637655	-0.024347	0.010010	0.000029	0.721827
0.792241	-0.089424	0.015014	0.000000	0.721753
0.602523	-0.058400	0.020019	0.000036	0.721748
0.726346	-0.082215	0.025024	0.000013	0.721744
0.721186	-0.079249	0.030029	0.000013	0.721749
0.710313	-0.080628	0.035034	0.000015	0.721742
0.685760	-0.071350	0.040038	0.000020	0.721752
0.504944	-0.041673	0.045043	0.000053	0.721747
0.387189	-0.021477	0.050048	0.000075	0.721746
0.436474	-0.027571	0.055053	0.000066	0.721751
0.654876	-0.070054	0.060058	0.000025	0.721744
0.698214	-0.075168	0.065062	0.000017	0.721749
0.491843	-0.041259	0.070067	0.000056	0.721744
0.466726	-0.036487	0.075072	0.000060	0.721745
0.476135	-0.036155	0.080077	0.000058	0.721749
0.348678	-0.114656	0.085082	0.000082	0.721550
0.401970	-0.179387	0.090086	0.000072	0.721441
0.416958	-0.184536	0.095091	0.000069	0.721437
0.512855	-0.200439	0.100096	0.000051	0.721439
0.459691	-0.189403	0.105101	0.000061	0.721442
0.342022	-0.171366	0.110106	0.000083	0.721437
0.378282	-0.174427	0.115110	0.000076	0.721443
0.343380	-0.276152	0.120115	0.000083	0.721231
0.417186	-0.343917	0.125120	0.000069	0.721124
0.572214	-0.368566	0.130125	0.000040	0.721130
0.455626	-0.351672	0.135130	0.000062	0.721122
0.405190	-0.339019	0.140134	0.000071	0.721130
0.431457	-0.412474	0.145139	0.000066	0.720995
0.540528	-0.490111	0.150144	0.000046	0.720880
0.471960	-0.474706	0.155149	0.000059	0.720886
0.463646	-0.476457	0.160154	0.000060	0.720880
0.423620	-0.521386	0.165158	0.000067	0.720778
0.172971	-0.597001	0.170163	0.000114	0.720541
0.252729	-0.611659	0.175168	0.000099	0.720541
0.338652	-0.623093	0.180173	0.000083	0.720548
0.311395	-0.691718	0.185178	0.000088	0.720404
0.186891	-0.759775	0.190182	0.000111	0.720226
0.353112	-0.791218	0.195187	0.000080	0.720223
0.429680	-0.803762	0.200192	0.000066	0.720225
0.262730	-0.929407	0.205197	0.000097	0.719919
0.250300	-0.937115	0.210202	0.000099	0.719900
0.609582	-0.997830	0.215206	0.000033	0.719906
0.409465	-1.089741	0.220211	0.000070	0.719655
0.516672	-1.134511	0.225216	0.000050	0.719604
0.537062	-1.134479	0.230221	0.000046	0.719612
0.257970	-1.254425	0.235226	0.000098	0.719277
0.322364	-1.265714	0.240230	0.000086	0.719278
0.211447	-1.278669	0.245235	0.000107	0.719213
0.138922	-1.391200	0.250240	0.000120	0.718966
0.362314	-1.427959	0.255245	0.000078	0.718972
0.179376	-1.494444	0.260250	0.000112	0.718777
0.316248	-1.582709	0.265254	0.000087	0.718651
0.199925	-1.575968	0.270259	0.000109	0.718623
0.049283	-1.682626	0.275264	0.000137	0.718360
0.170596	-1.700536	0.280269	0.000114	0.718367
0.129348	-1.811970	0.285274	0.000122	0.718133
0.071776	-1.855352	0.290278	0.000132	0.718027
-0.145899	-1.869183	0.295283	0.000173	0.717923
-0.257512	-1.957308	0.300288	0.000194	0.717710
-0.381179	-1.932219	0.305293	0.000217	0.717716
-0.439617	-2.086511	0.310298	0.000227	0.717391
-0.165240	-2.136309	0.315302	0.000176	0.717389
-0.358383	-2.210028	0.320307	0.000212	0.717175
-0.868963	-2.163729	0.325312	0.000307	0.717087
-1.561756	-2.101260	0.330317	0.000436	0.716967
-2.724515	-2.001169	0.335322	0.000653	0.716755
-2.281513	-2.077062	0.340326	0.000570	0.716761
-2.674395	-2.081744	0.345331	0.000643	0.716613
-3.924350	-1.940281	0.350336	0.000876	0.716453
-2.957342	-2.110544	0.355341	0.000696	0.716457
-3.436178	-2.072055	0.360346	0.000785	0.716364
-4.579656	-1.982900	0.365350	0.000998	0.716137
-3.898556	-2.106020	0.370355	0.000871	0.716134
-4.320282	-2.031229	0.375360	0.000949	0.716133
-4.503173	-2.093296	0.380365	0.000983	0.715946
-5.289858	-1.984215	0.385370	0.001130	0.715885
-5.340397	-1.971843	0.390374	0.001139	0.715891
-4.953679	-2.041027	0.395379	0.001067	0.715891
-5.534327	-2.089964	0.400384	0.001175	0.715589
-5.865801	-2.048491	0.405389	0.001237	0.715554
-6.073428	-2.015932	0.410394	0.001275	0.715546
-6.166292	-1.996612	0.415398	0.001292	0.715551
-6.214962	-2.068221	0.420403	0.001301	0.715392
-6.981317	-2.012353	0.425408	0.001444	0.715232
-6.628273	-2.070504	0.430413	0.001378	0.715242
-7.209344	-1.973302	0.435418	0.001486	0.715229
-6.755303	-2.050902	0.440422	0.001402	0.715236
-6.819330	-2.180003	0.445427	0.001414	0.714957
-8.217858	-1.956438	0.450432	0.001674	0.714907
-8.116206	-1.970083	0.455437	0.001655	0.714916
-7.779540	-2.034445	0.460442	0.001592	0.714907
-8.032478	-1.986453	0.465446	0.001639	0.714913
-8.079696	-2.060290	0.470451	0.001648	0.714750
-8.748249	-2.012878	0.475456	0.001772	0.714608
-8.498695	-2.054250	0.480461	0.001726	0.714614
-8.994397	-1.968002	0.485466	0.001818	0.714610
-8.552468	-2.044983	0.490470	0.001736	0.714614
-8.375926	-2.084356	0.495475	0.001703	0.714598
-9.752313	-2.001012	0.500480	0.001959	0.714277
-9.696321	-2.007116	0.505485	0.001949	0.714285
-9.715980	-2.005833	0.510490	0.001952	0.714280
-9.634468	-2.018252	0.515494	0.001937	0.714285
-9.923120	-1.968574	0.520499	0.001991	0.714281
-9.980620	-1.960352	0.525504	0.002001	0.714277
-9.835741	-2.068415	0.530509	0.001974	0.714114
-11.128518	-1.910621	0.535514	0.002215	0.713970
-10.693201	-1.985722	0.540518	0.002134	0.713975
-10.561213	-2.011770	0.545523	0.002109	0.713970
-11.257959	-1.888519	0.550528	0.002239	0.713968
-10.669998	-1.989834	0.555533	0.002129	0.713975
-10.151328	-2.085442	0.560538	0.002033	0.713969
-10.868344	-2.086791	0.565542	0.002166	0.713713
-11.680764	-1.969585	0.570547	0.002317	0.713658
-11.669128	-1.974111	0.575552	0.002315	0.713653
-11.255366	-2.045336	0.580557	0.002238	0.713658
-11.924799	-1.929971	0.585562	0.002363	0.713651
-11.576855	-1.986721	0.590566	0.002298	0.713661
-11.303360	-2.061456	0.595571	0.002247	0.713610
-12.675333	-1.941840	0.600576	0.002502	0.713362
-12.276703	-2.008567	0.605581	0.002428	0.713370
-12.531982	-1.968322	0.610586	0.002475	0.713360
-12.462293	-1.977539	0.615590	0.002462	0.713366
-12.645583	-1.946432	0.620595	0.002496	0.713363
-12.630725	-1.948980	0.625600	0.002494	0.713364
-12.130093	-2.073551	0.630605	0.002400	0.713293
-13.599320	-1.947330	0.635610	0.002674	0.713024
-13.393474	-1.981319	0.640614	0.002635	0.713029
-13.444832	-1.972698	0.645619	0.002645	0.713028
-13.403870	-1.981074	0.650624	0.002637	0.713026
-13.240985	-2.008781	0.655629	0.002607	0.713029
-13.415367	-1.979809	0.660634	0.002639	0.713025
-13.508504	-1.968410	0.665638	0.002657	0.713015
-14.128103	-2.007037	0.670643	0.002772	0.712718
-14.519378	-1.940162	0.675648	0.002845	0.712713
-14.446765	-1.949512	0.680653	0.002831	0.712720
-14.569512	-1.932129	0.685658	0.002854	0.712711
-14.534341	-1.935279	0.690662	0.002847	0.712718
-14.236048	-1.990917	0.695667	0.002792	0.712713
-14.322851	-1.976018	0.700672	0.002808	0.712712
-14.591624	-2.014697	0.705677	0.002858	0.712539
-15.560386	-1.918009	0.710682	0.003038	0.712388
-15.018184	-2.011583	0.715686	0.002937	0.712394
-15.038440	-2.008071	0.720691	0.002941	0.712394
-15.398621	-1.947869	0.725696	0.003008	0.712387
-14.756433	-2.057221	0.730701	0.002888	0.712397
-15.225450	-1.977980	0.735706	0.002975	0.712388
-15.728232	-1.983185	0.740710	0.003069	0.712200
-16.119566	-1.965219	0.745715	0.003142	0.712097
-16.132889	-1.967368	0.750720	0.003144	0.712088
-16.102204	-1.969055	0.755725	0.003138	0.712095
-16.165155	-1.962087	0.760730	0.003150	0.712087
-15.880313	-2.010589	0.765734	0.003097	0.712092
-16.088986	-1.973034	0.770739	0.003136	0.712092
-16.607205	-1.960605	0.775744	0.003232	0.711933
-17.245382	-1.928699	0.780749	0.003351	0.711770
-17.043673	-1.969946	0.785754	0.003313	0.711760
-17.277043	-1.925171	0.790758	0.003357	0.711766
-16.875408	-1.996365	0.795763	0.003282	0.711767
-16.961940	-1.984097	0.800768	0.003298	0.711761
-17.197957	-1.937010	0.805773	0.003342	0.711771
-17.076008	-1.974771	0.810778	0.003319	0.711739
-17.664938	-2.009691	0.815782	0.003429	0.711461
-17.980492	-1.953832	0.820787	0.003487	0.711460
-18.469789	-1.867953	0.825792	0.003578	0.711457
-17.778721	-1.986968	0.830797	0.003450	0.711466
-17.826454	-1.983060	0.835802	0.003458	0.711457
-18.447095	-1.871584	0.840806	0.003574	0.711459
-17.932577	-1.961644	0.845811	0.003478	0.711462
-18.296794	-2.003963	0.850816	0.003546	0.711248
-19.141859	-1.905027	0.855821	0.003703	0.711145
-18.992238	-1.934368	0.860826	0.003675	0.711140
-18.712433	-1.982839	0.865830	0.003623	0.711143
-18.886095	-1.951638	0.870835	0.003655	0.711143
-19.118679	-1.914122	0.875840	0.003699	0.711136
-18.541316	-2.011355	0.880845	0.003591	0.711147
-18.888722	-2.022288	0.885850	0.003656	0.711002
-19.639295	-1.952484	0.890854	0.003795	0.710874
-19.313091	-2.008053	0.895859	0.003735	0.710880
-19.558326	-1.969571	0.900864	0.003780	0.710869
-19.460993	-1.982204	0.905869	0.003762	0.710879
-19.619591	-1.958613	0.910874	0.003791	0.710870
-19.370004	-2.021601	0.915878	0.003745	0.710833
-20.180302	-2.023992	0.920883	0.003896	0.710540
-20.563588	-1.959655	0.925888	0.003967	0.710532
-20.602566	-1.950539	0.930893	0.003974	0.710536
-20.569903	-1.958567	0.935898	0.003968	0.710532
-20.473043	-1.972721	0.940902	0.003950	0.710538
-20.313388	-1.999472	0.945907	0.003920	0.710542
-20.354716	-2.045699	0.950912	0.003928	0.710435
-21.185485	-2.003303	0.955917	0.004082	0.710224
-21.482290	-1.953045	0.960922	0.004138	0.710219
-21.540680	-1.942346	0.965926	0.004148	0.710220
-21.346879	-1.975145	0.970931	0.004112	0.710223
-21.602181	-1.933143	0.975936	0.004160	0.710216
-21.219487	-1.995815	0.980941	0.004088	0.710227
-21.273403	-2.037820	0.985946	0.004098	0.710124
-22.394016	-1.950746	0.990950	0.004307	0.709899
-22.227430	-1.980570	0.995955	0.004276	0.709899
-22.745812	-1.890471	1.000960	0.004372	0.709895
-22.434501	-1.941675	1.005965	0.004314	0.709904
-22.500078	-1.934927	1.010970	0.004327	0.709894
-22.791308	-1.881327	1.015974	0.004381	0.709897
-22.441582	-1.943164	1.020979	0.004316	0.709898
-22.848939	-1.963530	1.025984	0.004391	0.709713
-23.480464	-1.905716	1.030989	0.004509	0.709603
-23.186361	-1.962598	1.035994	0.004454	0.709594
-23.269440	-1.945158	1.040998	0.004469	0.709600
-23.282477	-1.942112	1.046003	0.004472	0.709601
-23.223071	-1.958143	1.051008	0.004461	0.709591
-23.127191	-1.970020	1.056013	0.004443	0.709601
-23.454662	-1.978558	1.061018	0.004504	0.709467
-24.320222	-1.924924	1.066022	0.004665	0.709266
-23.539112	-2.063179	1.071027	0.004519	0.709268
-24.315180	-1.927812	1.076032	0.004664	0.709262
-24.132918	-1.954580	1.081037	0.004630	0.709274
-23.960011	-1.989120	1.086042	0.004597	0.709267
-24.251706	-1.937465	1.091046	0.004652	0.709266
-24.295357	-2.001309	1.096051	0.004660	0.709123
-25.382456	-1.890828	1.101056	0.004862	0.708956
-24.795902	-1.992228	1.106061	0.004753	0.708963
-24.968947	-1.964408	1.111066	0.004785	0.708957
-25.062446	-1.947997	1.116070	0.004802	0.708956
-24.766107	-1.998921	1.121075	0.004747	0.708960
-25.257079	-1.915608	1.126080	0.004838	0.708952
-25.094912	-1.994740	1.131085	0.004808	0.708852
-26.021878	-1.935442	1.136090	0.004981	0.708640
-26.051496	-1.929286	1.141094	0.004986	0.708642
-25.865369	-1.961075	1.146099	0.004952	0.708644
-26.201829	-1.905102	1.151104	0.005014	0.708637
-25.810504	-1.969412	1.156109	0.004941	0.708648
-26.132056	-1.916602	1.161114	0.005001	0.708639
-26.022013	-1.941534	1.166118	0.004980	0.708628
-26.231711	-2.040460	1.171123	0.005019	0.708355
-26.931196	-1.920521	1.176128	0.005150	0.708346
-26.968174	-1.908263	1.181133	0.005156	0.708357
-26.497018	-1.996270	1.186138	0.005069	0.708349
-26.816465	-1.937834	1.191142	0.005128	0.708352
-26.720843	-1.953805	1.196147	0.005110	0.708355
-26.935849	-1.938484	1.201152	0.005150	0.708309
-27.483043	-1.985134	1.206157	0.005252	0.708020
-27.790042	-1.934250	1.211162	0.005309	0.708012
-28.014921	-1.893720	1.216166	0.005351	0.708013
-27.326969	-2.012387	1.221171	0.005223	0.708021
-28.045912	-1.887962	1.226176	0.005357	0.708014
-27.947734	-1.901704	1.231181	0.005338	0.708022
-27.585110	-1.970600	1.236186	0.005271	0.708013
-28.286131	-1.980465	1.241190	0.005401	0.707743
-29.007294	-1.870351	1.246195	0.005535	0.707706
-28.942538	-1.885143	1.251200	0.005523	0.707700
-28.373082	-1.981759	1.256205	0.005417	0.707710
-28.682493	-1.931337	1.261210	0.005475	0.707700
-28.900296	-1.893469	1.266214	0.005515	0.707699
-28.414451	-1.976467	1.271219	0.005425	0.707706
-28.910247	-1.958659	1.276224	0.005517	0.707564
-29.866209	-1.878456	1.281229	0.005695	0.707384
-29.373411	-1.969893	1.286234	0.005603	0.707376
-29.827367	-1.887869	1.291238	0.005687	0.707379
-29.642654	-1.918984	1.296243	0.005653	0.707383
-29.474148	-1.951683	1.301248	0.005622	0.707377
-29.509306	-1.942169	1.306253	0.005628	0.707384
-29.814891	-1.904055	1.311258	0.005685	0.707351
-30.462314	-1.922325	1.316262	0.005805	0.707083
-30.185428	-1.969599	1.321267	0.005754	0.707087
-30.491510	-1.920269	1.326272	0.005811	0.707077
-30.371360	-1.935485	1.331277	0.005788	0.707090
-30.496011	-1.916590	1.336282	0.005811	0.707083
-30.638933	-1.890900	1.341286	0.005838	0.707084
-30.354057	-1.942320	1.346291	0.005785	0.707082
-31.005331	-1.990005	1.351296	0.005906	0.706754
-31.333905	-1.928541	1.356301	0.005967	0.706760
-31.565215	-1.889194	1.361306	0.006010	0.706756
-31.421688	-1.914797	1.366310	0.005983	0.706756
-31.209987	-1.950843	1.371315	0.005944	0.706759
-31.543294	-1.896384	1.376320	0.006006	0.706750
-31.405345	-1.916253	1.381325	0.005980	0.706759
-31.394385	-2.044964	1.386330	0.005978	0.706505
-32.145256	-1.941511	1.391334	0.006118	0.706444
-32.157879	-1.935707	1.396339	0.006120	0.706451
-32.108082	-1.948681	1.401344	0.006111	0.706443
-32.258382	-1.919306	1.406349	0.006139	0.706448
-32.293402	-1.917317	1.411354	0.006145	0.706440
-32.358562	-1.905410	1.416358	0.006157	0.706441
-32.581958	-2.012668	1.421363	0.006199	0.706145
-32.959555	-1.956015	1.426368	0.006269	0.706124
-33.228051	-1.903708	1.431373	0.006319	0.706133
-33.202352	-1.911259	1.436378	0.006314	0.706127
-33.071880	-1.935429	1.441382	0.006290	0.706125
-33.145185	-1.919508	1.446387	0.006303	0.706131
-33.167070	-1.920285	1.451392	0.006307	0.706122
-33.304761	-2.011859	1.456397	0.006333	0.705888
-33.729890	-1.949211	1.461402	0.006412	0.705862
-34.174510	-1.869738	1.466406	0.006495	0.705863
-33.588753	-1.972974	1.471411	0.006386	0.705865
-33.973401	-1.907801	1.476416	0.006457	0.705858
-34.087023	-1.883878	1.481421	0.006478	0.705866
-33.743435	-1.974602	1.486426	0.006414	0.705807
-34.680123	-1.949095	1.491430	0.006589	0.705522
-34.635606	-1.953365	1.496435	0.006580	0.705530
-35.232523	-1.850464	1.501440	0.006691	0.705523
-34.696725	-1.942625	1.506445	0.006592	0.705530
-34.605419	-1.961675	1.511450	0.006574	0.705524
-35.025125	-1.887689	1.516454	0.006653	0.705523
-34.683973	-1.981067	1.521459	0.006589	0.705457
-35.614124	-1.938737	1.526464	0.006762	0.705209
-35.623719	-1.933052	1.531469	0.006764	0.705217
-35.791631	-1.905309	1.536474	0.006795	0.705213
-35.540333	-1.952028	1.541478	0.006748	0.705209
-35.436460	-1.967463	1.546483	0.006729	0.705215
-35.982857	-1.876085	1.551488	0.006830	0.705203
-35.611601	-1.976560	1.556493	0.006761	0.705134
-36.386942	-1.961727	1.561498	0.006906	0.704886
-36.772807	-1.892219	1.566502	0.006977	0.704887
-36.698855	-1.903446	1.571507	0.006964	0.704892
-36.515418	-1.940276	1.576512	0.006929	0.704883
-36.593988	-1.922723	1.581517	0.006944	0.704891
-36.712044	-1.903827	1.586522	0.006966	0.704886
-36.468478	-1.960521	1.591526	0.006920	0.704860
-36.919256	-2.012640	1.596531	0.007004	0.704593
-37.567369	-1.902150	1.601536	0.007125	0.704583
-37.483265	-1.911430	1.606541	0.007109	0.704595
-37.068997	-1.986893	1.611546	0.007032	0.704591
-37.339645	-1.939901	1.616550	0.007082	0.704589
-37.304057	-1.943476	1.621555	0.007076	0.704595
-37.023891	-2.076560	1.626560	0.007023	0.704427
-38.307836	-1.926976	1.631565	0.007262	0.704268
-38.186552	-1.952568	1.636570	0.007240	0.704260
-38.102758	-1.966868	1.641574	0.007224	0.704261
-38.203763	-1.945860	1.646579	0.007243	0.704267
-38.371392	-1.923156	1.651584	0.007274	0.704253
-38.384963	-1.916343	1.656589	0.007276	0.704262
-38.503946	-1.993590	1.661594	0.007299	0.704063
-39.745594	-1.826306	1.666598	0.007530	0.703954
-39.136413	-1.931955	1.671603	0.007416	0.703961
-39.105713	-1.941821	1.676608	0.007410	0.703952
-39.179723	-1.925511	1.681613	0.007424	0.703958
-39.276121	-1.910820	1.686618	0.007442	0.703953
-39.200515	-1.924823	1.691622	0.007428	0.703952
-38.845998	-2.052088	1.696627	0.007362	0.703823
-40.421389	-1.866436	1.701632	0.007655	0.703631
-40.016824	-1.934408	1.706637	0.007580	0.703640
-39.851148	-1.965282	1.711642	0.007549	0.703637
-40.089954	-1.925200	1.716646	0.007593	0.703632
-39.890489	-1.957804	1.721651	0.007556	0.703638
-39.833563	-1.973388	1.726656	0.007545	0.703628
-40.177062	-1.996475	1.731661	0.007609	0.703457
-41.173667	-1.876380	1.736666	0.007795	0.703341
-40.982470	-1.911804	1.741670	0.007759	0.703339
-40.495177	-1.995844	1.746675	0.007668	0.703345
-41.066398	-1.897768	1.751680	0.007775	0.703337
-40.802008	-1.941099	1.756685	0.007725	0.703345
-40.563765	-1.986187	1.761690	0.007681	0.703340
-41.201153	-1.994677	1.766694	0.007800	0.703093
-41.987087	-1.895879	1.771699	0.007946	0.703010
-41.749998	-1.942654	1.776704	0.007902	0.703001
-41.178514	-2.039699	1.781709	0.007795	0.703011
-41.744583	-1.940606	1.786714	0.007900	0.703007
-41.966402	-1.901539	1.791718	0.007942	0.703006
-41.343337	-2.008902	1.796723	0.007826	0.703014
-42.399331	-1.971587	1.801728	0.008022	0.702709
-42.637681	-1.935520	1.806733	0.008066	0.702696
-42.469946	-1.966104	1.811738	0.008035	0.702695
-42.688952	-1.927807	1.816742	0.008076	0.702694
-42.624990	-1.935717	1.821747	0.008064	0.702701
-42.615013	-1.943425	1.826752	0.008062	0.702689
-42.256774	-2.011143	1.831757	0.007995	0.702681
-43.342169	-1.969434	1.836762	0.008197	0.702375
-43.708049	-1.907110	1.841766	0.008265	0.702369
-43.134886	-2.005583	1.846771	0.008159	0.702376
-43.331608	-1.974889	1.851776	0.008195	0.702368
-43.684939	-1.908702	1.856781	0.008261	0.702374
-43.399972	-1.960306	1.861786	0.008208	0.702373
-43.276330	-2.000671	1.866790	0.008185	0.702336
-43.995633	-1.998880	1.871795	0.008319	0.702080
-44.340832	-1.940589	1.876800	0.008383	0.702074
-44.031686	-1.994189	1.881805	0.008325	0.702077
-44.095726	-1.984140	1.886810	0.008337	0.702074
-44.341454	-1.941501	1.891814	0.008383	0.702072
-43.991319	-2.000326	1.896819	0.008317	0.702079
-44.197833	-2.054623	1.901824	0.008356	0.701895
-45.271270	-1.935371	1.906829	0.008556	0.701749
-44.755153	-2.027846	1.911834	0.008460	0.701749
-44.850154	-2.012623	1.916838	0.008477	0.701745
-45.291553	-1.930965	1.921843	0.008559	0.701751
-45.341320	-1.926816	1.926848	0.008568	0.701742
-45.015619	-1.980901	1.931853	0.008508	0.701750
-45.422486	-2.031815	1.936858	0.008584	0.701500
-46.458700	-1.879600	1.941862	0.008776	0.701435
-45.827867	-1.987907	1.946867	0.008659	0.701443
-45.761209	-2.004092	1.951872	0.008646	0.701435
-46.289779	-1.906851	1.956877	0.008745	0.701441
-46.151305	-1.932681	1.961882	0.008719	0.701439
-45.820445	-1.993434	1.966886	0.008657	0.701435
-46.272045	-2.024827	1.971891	0.008741	0.701209
-47.338905	-1.879075	1.976896	0.008940	0.701119
-46.803035	-1.971107	1.981901	0.008840	0.701126
-46.624128	-2.004301	1.986906	0.008807	0.701123
-47.157734	-1.910747	1.991910	0.008906	0.701120
-46.786035	-1.973195	1.996915	0.008837	0.701128
-46.961432	-1.978862	2.001920	0.008869	0.701053

-47.571942	-1.958525	2.011917	0.008983	0.700874
-47.675662	-1.940493	2.021914	0.009002	0.700874
-47.237413	-2.016176	2.031910	0.008920	0.700879
-47.780410	-1.920156	2.041907	0.009021	0.700877
-47.554399	-1.961463	2.051904	0.008979	0.700876
-47.703964	-1.934792	2.061901	0.009007	0.700876
-47.658525	-1.942548	2.071898	0.008998	0.700877
-47.609434	-1.950107	2.081894	0.008989	0.700879
-47.403413	-1.989045	2.091891	0.008950	0.700875
-47.555441	-1.961241	2.101888	0.008979	0.700877
-47.728498	-1.932387	2.111885	0.009011	0.700873
-47.093491	-1.964771	2.121882	0.008892	0.701037
-46.958688	-1.945790	2.131878	0.008867	0.701124
-47.047615	-1.931284	2.141875	0.008884	0.701122
-46.927390	-1.951835	2.151872	0.008861	0.701124
-46.757389	-1.984080	2.161869	0.008829	0.701120
-46.680362	-1.937232	2.171866	0.008815	0.701243
-45.843175	-1.990451	2.181862	0.008659	0.701438
-46.074647	-1.949252	2.191859	0.008702	0.701438
-45.994699	-1.964127	2.201856	0.008687	0.701437
-46.067820	-1.927269	2.211853	0.008700	0.701485
-45.167394	-1.959132	2.221850	0.008533	0.701746
-45.021611	-1.984008	2.231846	0.008505	0.701749
-45.329389	-1.930401	2.241843	0.008562	0.701746
-45.211897	-1.915124	2.251840	0.008540	0.701820
-44.369030	-1.940250	2.261837	0.008383	0.702073
-44.194555	-1.970163	2.271834	0.008351	0.702076
-44.267133	-1.955637	2.281830	0.008364	0.702079
-44.043141	-1.921033	2.291827	0.008322	0.702230
-43.450858	-1.957299	2.301824	0.008212	0.702371
-43.780222	-1.897180	2.311821	0.008273	0.702374
-43.415020	-1.952827	2.321818	0.008205	0.702393
-42.726251	-1.926964	2.331814	0.008077	0.702694
-42.517393	-1.963160	2.341811	0.008038	0.702696
-42.346359	-1.996209	2.351808	0.008006	0.702691
-42.484266	-1.925903	2.361805	0.008031	0.702784
-41.450332	-1.999222	2.371802	0.007839	0.703009
-41.664601	-1.960283	2.381798	0.007878	0.703010
-41.916273	-1.917035	2.391795	0.007925	0.703007
-41.072845	-1.931265	2.401792	0.007768	0.703282
-41.054185	-1.905327	2.411789	0.007764	0.703342
-40.575979	-1.990202	2.421786	0.007675	0.703343
-40.830430	-1.899499	2.431782	0.007722	0.703434
-39.913604	-1.962512	2.441779	0.007552	0.703637
-40.106728	-1.930172	2.451776	0.007587	0.703633
-40.175225	-1.917920	2.461773	0.007600	0.703634
-39.281894	-1.929329	2.471770	0.007434	0.703932
-39.026973	-1.963658	2.481766	0.007386	0.703955
-39.069792	-1.956256	2.491763	0.007394	0.703955
-38.956422	-1.923883	2.501760	0.007373	0.704061
-38.326094	-1.938276	2.511757	0.007255	0.704259
-38.227186	-1.955173	2.521754	0.007237	0.704261
-38.407571	-1.922742	2.531750	0.007270	0.704261
-37.573977	-1.909665	2.541747	0.007115	0.704587
-37.469622	-1.927416	2.551744	0.007095	0.704589
-37.540850	-1.915493	2.561741	0.007108	0.704588
-36.881163	-1.944738	2.571738	0.006985	0.704766
-36.748876	-1.905856	2.581734	0.006961	0.704892
-36.501368	-1.950834	2.591731	0.006914	0.704891
-36.508530	-1.928837	2.601728	0.006916	0.704933
-35.555524	-1.959939	2.611725	0.006738	0.705213
-35.387835	-1.989211	2.621722	0.006707	0.705214
-35.592328	-1.951863	2.631718	0.006745	0.705216
-35.441877	-1.909032	2.641715	0.006716	0.705356
-34.766161	-1.944057	2.651712	0.006591	0.705529
-34.944861	-1.912356	2.661709	0.006624	0.705529
-34.798160	-1.918427	2.671706	0.006596	0.705569
-33.867907	-1.935737	2.681702	0.006423	0.705868
-33.768451	-1.952572	2.691699	0.006404	0.705870
-33.842530	-1.941853	2.701696	0.006418	0.705865
-33.811875	-1.882612	2.711693	0.006412	0.705996
-33.090108	-1.943487	2.721690	0.006278	0.706132
-33.127026	-1.937527	2.731686	0.006284	0.706131
-33.062075	-1.921737	2.741683	0.006272	0.706187
-32.320681	-1.923090	2.751680	0.006134	0.706450
-32.186056	-1.948954	2.761677	0.006109	0.706446
-32.215233	-1.942080	2.771674	0.006114	0.706450
-31.749561	-1.903490	2.781670	0.006027	0.706694
-31.238614	-1.965776	2.791667	0.005932	0.706752
-31.446086	-1.928910	2.801664	0.005971	0.706752
-31.343327	-1.884149	2.811661	0.005951	0.706879
-30.535253	-1.926405	2.821658	0.005801	0.707084
-30.436326	-1.944155	2.831654	0.005782	0.707084
-30.374809	-1.954964	2.841651	0.005771	0.707084
-30.137285	-1.860363	2.851648	0.005726	0.707360
-29.451022	-1.972988	2.861645	0.005598	0.707379
-29.741533	-1.920426	2.871642	0.005652	0.707381
-29.284036	-1.907009	2.881638	0.005567	0.707572
-28.704045	-1.944388	2.891635	0.005459	0.707704
-28.908840	-1.909833	2.901632	0.005497	0.707701
-28.816762	-1.901424	2.911629	0.005480	0.707751
-27.682687	-1.971085	2.921626	0.005268	0.708017
-27.789590	-1.951718	2.931622	0.005288	0.708017
-27.911582	-1.931455	2.941619	0.005311	0.708015
-27.593383	-1.895691	2.951616	0.005251	0.708200
-26.914311	-1.941498	2.961613	0.005125	0.708351
-27.108364	-1.907730	2.971610	0.005161	0.708350
-26.982453	-1.918158	2.981606	0.005137	0.708374
-26.282795	-1.909871	2.991603	0.005007	0.708641
-26.374096	-1.894417	3.001600	0.005024	0.708639
-26.203655	-1.924989	3.011597	0.004992	0.708639
-25.676478	-1.896056	3.021594	0.004894	0.708886
-25.239787	-1.936802	3.031590	0.004812	0.708960
-25.124086	-1.957773	3.041587	0.004790	0.708960
-25.295959	-1.907504	3.051584	0.004822	0.708999
-24.580978	-1.901937	3.061581	0.004689	0.709266
-24.638960	-1.892579	3.071578	0.004700	0.709264
-24.548082	-1.907642	3.081574	0.004683	0.709266
-24.000072	-1.851946	3.091571	0.004581	0.709573
-23.732537	-1.889114	3.101568	0.004531	0.709595
-23.511555	-1.927714	3.111565	0.004489	0.709597
-23.261304	-1.895173	3.121562	0.004443	0.709751
-22.596114	-1.941448	3.131558	0.004319	0.709896
-23.048044	-1.861532	3.141555	0.004403	0.709895
-22.855243	-1.874429	3.151552	0.004367	0.709938
-22.093773	-1.870580	3.161549	0.004225	0.710217
-21.975183	-1.890814	3.171546	0.004203	0.710219
-21.589254	-1.958611	3.181542	0.004131	0.710221
-21.565434	-1.851023	3.191539	0.004126	0.710445
-21.019197	-1.903567	3.201536	0.004024	0.710535
-21.010989	-1.905537	3.211533	0.004023	0.710534
-21.150735	-1.835359	3.221530	0.004048	0.710625
-20.054209	-1.904459	3.231526	0.003844	0.710877
-20.178657	-1.885256	3.241523	0.003867	0.710871
-20.097131	-1.898373	3.251520	0.003852	0.710874
-19.654910	-1.872168	3.261517	0.003769	0.711084
-19.221913	-1.921875	3.271514	0.003689	0.711139
-19.195863	-1.924714	3.281510	0.003684	0.711143
-19.434729	-1.833347	3.291507	0.003728	0.711241
-18.470796	-1.897190	3.301504	0.003548	0.711456
-18.524983	-1.887533	3.311501	0.003558	0.711456
-18.578807	-1.877588	3.321498	0.003568	0.711457
-17.865481	-1.854367	3.331494	0.003435	0.711757
-17.628864	-1.893588	3.341491	0.003391	0.711763
-17.507616	-1.915897	3.351488	0.003369	0.711762
-17.447114	-1.831569	3.361485	0.003357	0.711952
-16.463032	-1.936649	3.371482	0.003174	0.712092
-16.681001	-1.896435	3.381478	0.003214	0.712095
-16.812577	-1.869812	3.391475	0.003239	0.712102
-15.779949	-1.910634	3.401472	0.003046	0.712387
-16.014019	-1.869200	3.411469	0.003090	0.712387
-15.766485	-1.912049	3.421466	0.003043	0.712390
-15.566976	-1.859033	3.431462	0.003006	0.712566
-14.791182	-1.923475	3.441459	0.002862	0.712714
-14.936879	-1.898769	3.451456	0.002889	0.712711
-15.148546	-1.856342	3.461453	0.002928	0.712721
-14.106202	-1.888900	3.471450	0.002734	0.713026
-14.036260	-1.901164	3.481446	0.002721	0.713027
-14.065728	-1.894970	3.491443	0.002726	0.713029
-13.715089	-1.872685	3.501440	0.002660	0.713198
-13.213596	-1.880910	3.511437	0.002567	0.713359
-12.951323	-1.926105	3.521434	0.002518	0.713362
-13.234693	-1.874280	3.531430	0.002571	0.713365
-12.490896	-1.878767	3.541427	0.002432	0.713620
-12.378668	-1.883116	3.551424	0.002411	0.713652
-12.380530	-1.882272	3.561421	0.002411	0.713653
-12.038919	-1.872098	3.571418	0.002348	0.713794
-11.437939	-1.889086	3.581414	0.002236	0.713974
-11.227999	-1.926094	3.591411	0.002196	0.713975
-11.367980	-1.902529	3.601408	0.002222	0.713972
-10.823237	-1.866318	3.611405	0.002121	0.714237
-10.311034	-1.935223	3.621402	0.002025	0.714282
-10.169368	-1.959201	3.631398	0.001999	0.714284
-10.175745	-1.959047	3.641395	0.002000	0.714283
-9.748647	-1.870206	3.651392	0.001920	0.714610
-9.415783	-1.930607	3.661389	0.001858	0.714609
-9.281560	-1.953613	3.671386	0.001833	0.714611
-9.334738	-1.888473	3.681382	0.001843	0.714721
-8.157516	-2.002358	3.691379	0.001623	0.714912
-8.301109	-1.977917	3.701376	0.001650	0.714910
-8.361910	-1.967634	3.711373	0.001661	0.714909
-8.214374	-1.942600	3.721370	0.001634	0.715011
-7.447575	-1.967209	3.731366	0.001491	0.715233
-7.347047	-1.986021	3.741363	0.001472	0.715232
-7.400027	-1.977172	3.751360	0.001482	0.715231
-7.065953	-1.964419	3.761357	0.001419	0.715374
-6.362104	-2.004910	3.771354	0.001288	0.715543
-6.639227	-1.954712	3.781350	0.001340	0.715545
-6.491101	-1.981413	3.791347	0.001312	0.715544
-6.060331	-1.923948	3.801344	0.001232	0.715811
-5.586095	-1.973960	3.811341	0.001143	0.715879
-5.328849	-2.018087	3.821338	0.001095	0.715883
-5.428015	-1.998843	3.831334	0.001114	0.715886
-4.880133	-1.982566	3.841331	0.001011	0.716112
-4.838610	-1.980255	3.851328	0.001004	0.716132
-4.618458	-2.019273	3.861325	0.000962	0.716132
-4.528006	-1.984764	3.871322	0.000945	0.716233
-3.750102	-2.013387	3.881318	0.000800	0.716451
-3.760869	-2.011112	3.891315	0.000802	0.716452
-4.179035	-1.938121	3.901312	0.000880	0.716449
-3.177634	-1.986265	3.911309	0.000694	0.716707
-2.956614	-2.001033	3.921306	0.000652	0.716756
-2.778393	-2.032342	3.931302	0.000619	0.716757
-2.800269	-2.006487	3.941299	0.000623	0.716801
-2.198434	-1.970073	3.951296	0.000511	0.717085
-2.029826	-2.000024	3.961293	0.000479	0.717085
-2.293111	-1.952809	3.971290	0.000528	0.717086
-1.870081	-1.921475	3.981286	0.000449	0.717297
-1.492813	-1.945476	3.991283	0.000379	0.717383
-1.438884	-1.955909	4.001280	0.000369	0.717382
-1.354923	-1.880224	4.011277	0.000353	0.717561
-1.542168	-1.774003	4.021274	0.000388	0.717705
-1.176182	-1.839031	4.031270	0.000319	0.717706
-1.085283	-1.702557	4.041267	0.000302	0.718008
-1.236921	-1.670601	4.051264	0.000330	0.718018
-1.466580	-1.509615	4.061261	0.000373	0.718255
-1.070458	-1.529233	4.071258	0.000299	0.718356
-0.855139	-1.455362	4.081254	0.000259	0.718578
-0.845416	-1.422211	4.091251	0.000257	0.718647
-0.737829	-1.301499	4.101248	0.000236	0.718923
-0.519421	-1.307360	4.111245	0.000196	0.718989
-0.494788	-1.167447	4.121242	0.000191	0.719273
-0.411271	-1.114191	4.131238	0.000175	0.719408
-0.551129	-0.991288	4.141235	0.000201	0.719601
-0.483142	-0.871744	4.151232	0.000188	0.719861
-0.425965	-0.790058	4.161229	0.000177	0.720042
-0.284417	-0.712819	4.171226	0.000151	0.720244
-0.211154	-0.575477	4.181222	0.000137	0.720541
-0.201919	-0.450459	4.191219	0.000135	0.720790
-0.234621	-0.338109	4.201216	0.000141	0.721000
-0.163897	-0.242199	4.211213	0.000128	0.721214
-0.208904	-0.094485	4.221210	0.000136	0.721489
-0.050622	0.013425	4.231206	0.000106	0.721756
0.038607	0.161171	4.241203	0.000089	0.722078
0.000000	0.321199	4.251200	0.000096	0.722379

0.096543	0.930967	4.256205	0.000078	0.723609
0.202938	2.171800	4.261210	0.000057	0.726075
0.430291	3.986404	4.266214	0.000014	0.729690
0.644380	6.359749	4.271219	-0.000028	0.734363
0.886046	9.226008	4.276224	-0.000075	0.739961
1.325668	12.551326	4.281229	-0.000159	0.746456
1.783073	16.323990	4.286234	-0.000247	0.753744
2.122133	20.523935	4.291238	-0.000313	0.761718
2.424546	25.130039	4.296243	-0.000372	0.770346
2.651936	30.111222	4.301248	-0.000418	0.779537
3.316954	35.369062	4.306253	-0.000545	0.789258
3.848285	40.969466	4.311258	-0.000648	0.799426
4.391456	46.867205	4.316262	-0.000753	0.809990
5.224389	53.009062	4.321267	-0.000912	0.820928
6.207216	59.398134	4.326272	-0.001099	0.832189
6.861595	66.078114	4.331277	-0.001225	0.843690
7.393731	73.000706	4.336282	-0.001329	0.855403
8.144078	80.083936	4.341286	-0.001473	0.867283
8.930811	87.364501	4.346291	-0.001625	0.879331
9.732149	94.803430	4.351296	-0.001779	0.891471
10.459690	102.433015	4.356301	-0.001919	0.903727
11.170442	110.205427	4.361306	-0.002057	0.916035
11.536974	118.147340	4.366310	-0.002130	0.928346
12.183845	126.171362	4.371315	-0.002256	0.940693
12.864789	134.284778	4.376320	-0.002388	0.953022
13.376910	142.517346	4.381325	-0.002489	0.965325
14.145125	150.784559	4.386330	-0.002637	0.977587
14.714333	159.175100	4.391334	-0.002749	0.989825
15.267756	167.617986	4.396339	-0.002857	1.001982
15.472792	176.142606	4.401344	-0.002901	1.014024
16.094343	184.640024	4.406349	-0.003023	1.025986
17.011666	193.125315	4.411354	-0.003199	1.037863
17.344523	201.731542	4.416358	-0.003267	1.049632
17.785974	210.342225	4.421363	-0.003354	1.061301
18.924734	218.858722	4.426368	-0.003572	1.072878
19.599794	227.468567	4.431373	-0.003703	1.084348
20.197807	236.108651	4.436378	-0.003821	1.095720
20.729974	244.748058	4.441382	-0.003925	1.106959
21.384523	253.391007	4.446387	-0.004053	1.118116
21.628827	262.078394	4.451392	-0.004104	1.129129
22.295064	270.712146	4.456397	-0.004234	1.140060
23.294412	279.302709	4.461402	-0.004426	1.150903
24.250391	287.871177	4.466406	-0.004609	1.161609
24.781001	296.511793	4.471411	-0.004714	1.172215
25.353675	305.112366	4.476416	-0.004826	1.182687
26.040706	313.717197	4.481421	-0.004960	1.193095
26.804576	322.267721	4.486426	-0.005107	1.203364
27.198075	330.890107	4.491430	-0.005186	1.213556
28.063714	339.419955	4.496435	-0.005353	1.223649
28.625597	348.008536	4.501440	-0.005463	1.233667
29.421096	356.520474	4.506445	-0.005617	1.243562
30.341968	365.006909	4.511450	-0.005794	1.253373
30.786236	373.547019	4.516454	-0.005883	1.263078
31.162421	382.110664	4.521459	-0.005958	1.272721
31.789908	390.576499	4.526464	-0.006081	1.282231
32.438321	399.059288	4.531469	-0.006207	1.291693
33.002372	407.536232	4.536474	-0.006318	1.301064
33.417218	416.085138	4.541478	-0.006401	1.310419
33.953585	424.604077	4.546483	-0.006506	1.319696
34.539347	432.994356	4.551488	-0.006621	1.328780
34.965182	441.434136	4.556493	-0.006705	1.337827
35.580267	449.810402	4.561498	-0.006826	1.346779
36.134091	458.210845	4.566502	-0.006934	1.355686
36.870244	466.555502	4.571507	-0.007077	1.364508
37.442767	474.928478	4.576512	-0.007189	1.373275
38.154177	483.280318	4.581517	-0.007327	1.381987
38.462858	491.699135	4.586522	-0.007390	1.390645
38.767826	500.085591	4.591526	-0.007452	1.399216
39.476038	508.396742	4.596531	-0.007590	1.407725
40.076519	516.728602	4.601536	-0.007707	1.416187
40.505656	525.070817	4.606541	-0.007792	1.424580
40.988983	533.419889	4.611546	-0.007888	1.432939
41.437715	541.732252	4.616550	-0.007977	1.441207
42.066533	550.043453	4.621555	-0.008099	1.449457
42.345427	558.379551	4.626560	-0.008157	1.457627
42.874976	566.669402	4.631565	-0.008261	1.465747
43.405645	575.007455	4.636570	-0.008365	1.473869
43.749238	583.293627	4.641574	-0.008435	1.481867
44.366605	591.545500	4.646579	-0.008555	1.489832
44.665242	599.849943	4.651584	-0.008616	1.497754
44.916262	608.132442	4.656589	-0.008668	1.505607
45.379009	616.410891	4.661594	-0.008760	1.513448
45.767306	624.654874	4.666598	-0.008838	1.521205
46.428790	632.885442	4.671603	-0.008966	1.528950
46.848643	641.142347	4.676608	-0.009050	1.536645
47.433225	649.370261	4.681613	-0.009164	1.544299
47.705306	657.668347	4.686618	-0.009220	1.551933
47.864377	665.936792	4.691622	-0.009255	1.559486
48.401993	674.139160	4.696627	-0.009361	1.566998
48.849204	682.370679	4.701632	-0.009449	1.574487
49.234830	690.596649	4.706637	-0.009527	1.581927
49.628518	698.823429	4.711642	-0.009605	1.589333
50.218784	707.011388	4.716646	-0.009721	1.596699
50.667708	715.225067	4.721651	-0.009810	1.604033
51.076479	723.441801	4.726656	-0.009891	1.611331
51.549229	731.660548	4.731661	-0.009985	1.618606
51.616966	739.916815	4.736666	-0.010003	1.625825
52.045475	748.167907	4.741670	-0.010088	1.633057
52.556181	756.347368	4.746675	-0.010188	1.640207
52.864454	764.531685	4.751680	-0.010251	1.647302
53.210429	772.753512	4.756685	-0.010321	1.654404
53.569356	780.930668	4.761690	-0.010393	1.661439
53.880679	789.116462	4.766694	-0.010457	1.668445
54.631782	797.267283	4.771699	-0.010602	1.675451
54.896967	805.448470	4.776704	-0.010657	1.682388
55.304925	813.630736	4.781709	-0.010738	1.689317
55.794873	821.808874	4.786714	-0.010835	1.696225
56.186877	829.974237	4.791718	-0.010913	1.703081
56.658191	838.158001	4.796723	-0.011006	1.709934
56.967524	846.356547	4.801728	-0.011069	1.716752
57.267612	854.530039	4.806733	-0.011130	1.723521
57.647192	862.685004	4.811738	-0.011206	1.730258
57.987054	870.862709	4.816742	-0.011275	1.736982
58.591096	878.989208	4.821747	-0.011393	1.743672
58.750248	887.181086	4.826752	-0.011428	1.750334
59.177849	895.353904	4.831757	-0.011513	1.756988
59.419687	903.527672	4.836762	-0.011563	1.763594
59.694001	911.681258	4.841766	-0.011620	1.770164
60.005445	919.868081	4.846771	-0.011683	1.776740
60.445913	927.996722	4.851776	-0.011771	1.783262
60.867792	936.155904	4.856781	-0.011855	1.789782
61.355202	944.334724	4.861786	-0.011951	1.796301
61.523188	952.474591	4.866790	-0.011987	1.802727
61.936814	960.605706	4.871795	-0.012070	1.809153
62.221330	968.757081	4.876800	-0.012128	1.815557
62.943959	976.829982	4.881805	-0.012268	1.821929
63.376474	984.972323	4.886810	-0.012354	1.828299
63.352442	993.176935	4.891814	-0.012355	1.834639
64.042972	1001.261168	4.896819	-0.012489	1.840950
64.586761	1009.367008	4.901824	-0.012595	1.847238
65.026055	1017.531933	4.906829	-0.012683	1.853538
65.372558	1025.682483	4.911834	-0.012752	1.859795
65.627914	1033.820863	4.916838	-0.012805	1.866010
66.061512	1041.994514	4.921843	-0.012891	1.872252
66.081884	1050.164030	4.926848	-0.012901	1.878423
66.403011	1058.274349	4.931853	-0.012966	1.884563
66.857954	1066.390039	4.936858	-0.013056	1.890703
67.103566	1074.529834	4.941862	-0.013107	1.896817
67.542154	1082.634134	4.946867	-0.013194	1.902906
67.960909	1090.742768	4.951872	-0.013277	1.908977
68.187320	1098.902489	4.956877	-0.013325	1.915045
68.541859	1107.002659	4.961882	-0.013396	1.921064
68.773455	1115.121836	4.966886	-0.013445	1.927064
69.427612	1123.210747	4.971891	-0.013572	1.933070
69.473465	1131.372068	4.976896	-0.013586	1.939044
69.806792	1139.473376	4.981901	-0.013653	1.944986
70.341969	1147.601521	4.986906	-0.013758	1.950952
70.451976	1155.766556	4.991910	-0.013784	1.956881
70.835204	1163.851070	4.996915	-0.013861	1.962762
71.202351	1171.928940	5.001920	-0.013934	1.968620
71.611419	1180.046712	5.006925	-0.014016	1.974493
71.872516	1188.152351	5.011930	-0.014070	1.980324
72.121631	1196.241859	5.016934	-0.014122	1.986125
72.628645	1204.372016	5.021939	-0.014221	1.991965
72.685786	1212.498583	5.026944	-0.014237	1.997739
73.109564	1220.579314	5.031949	-0.014322	2.003501
73.464664	1228.685657	5.036954	-0.014393	2.009258
73.599788	1236.819002	5.041958	-0.014423	2.014994
73.829771	1244.936907	5.046963	-0.014472	2.020713
74.079349	1253.028648	5.051968	-0.014523	2.026400
74.336475	1261.163069	5.056973	-0.014577	2.032101
74.858371	1269.227217	5.061978	-0.014679	2.037764
75.211785	1277.291455	5.066982	-0.014750	2.043395
75.798955	1285.371946	5.071987	-0.014865	2.049045
76.153144	1293.476979	5.076992	-0.014936	2.054672
76.296062	1301.596835	5.081997	-0.014968	2.060273
76.694853	1309.679417	5.087002	-0.015048	2.065859
76.777028	1317.816953	5.092006	-0.015068	2.071435
77.213952	1325.914247	5.097011	-0.015155	2.077004
77.450711	1333.995258	5.102016	-0.015205	2.082528
77.791774	1342.091051	5.107021	-0.015273	2.088057
78.311862	1350.181206	5.112026	-0.015376	2.093585
78.482088	1358.281860	5.117030	-0.015413	2.099071
79.120832	1366.332065	5.122035	-0.015537	2.104555
79.139774	1374.502251	5.127040	-0.015546	2.110045
79.329898	1382.660627	5.132045	-0.015587	2.115529
79.799129	1390.702307	5.137050	-0.015679	2.120947
80.045741	1398.760405	5.142054	-0.015730	2.126342
80.384580	1406.860701	5.147059	-0.015799	2.131759
80.851041	1414.915463	5.152064	-0.015891	2.137145
81.034880	1423.007584	5.157069	-0.015931	2.142515
81.244316	1431.110572	5.162074	-0.015975	2.147880
81.596865	1439.193815	5.167078	-0.016046	2.153233
81.927340	1447.275609	5.172083	-0.016113	2.158570
81.981199	1455.368915	5.177088	-0.016128	2.163875
82.165249	1463.468138	5.182093	-0.016168	2.169183
82.673981	1471.528211	5.187098	-0.016268	2.174483
82.971598	1479.594816	5.192102	-0.016329	2.179754
83.233649	1487.685987	5.197107	-0.016383	2.185025
83.459628	1495.791385	5.202112	-0.016430	2.190290
83.812144	1503.887666	5.207117	-0.016501	2.195547
84.096964	1511.957601	5.212122	-0.016559	2.200768
84.182151	1520.033481	5.217126	-0.016581	2.205963
84.909402	1528.073381	5.222131	-0.016721	2.211181
85.112956	1536.180578	5.227136	-0.016765	2.216382
85.257397	1544.260394	5.232141	-0.016797	2.221548
85.526851	1552.350930	5.237146	-0.016852	2.226720
85.730940	1560.436161	5.242150	-0.016896	2.231870
86.192228	1568.507207	5.247155	-0.016987	2.237023
86.520452	1576.558416	5.252160	-0.017053	2.242139
86.752892	1584.640387	5.257165	-0.017102	2.247255
87.069623	1592.734178	5.262170	-0.017166	2.252373
87.278480	1600.802609	5.267174	-0.017210	2.257455
87.555179	1608.881704	5.272179	-0.017267	2.262538
87.825304	1616.964078	5.277184	-0.017323	2.267611
88.082378	1625.111188	5.282189	-0.017376	2.272711
88.597660	1633.158157	5.287194	-0.017477	2.277760
88.761333	1641.201918	5.292198	-0.017513	2.282766
89.043616	1649.270570	5.297203	-0.017571	2.287786
89.261507	1657.351355	5.302208	-0.017617	2.292797
89.557812	1665.407257	5.307213	-0.017677	2.297789
90.028855	1673.456892	5.312218	-0.017770	2.302780
90.161416	1681.536388	5.317222	-0.017800	2.307751
90.654481	1689.617198	5.322227	-0.017898	2.312741
90.995901	1697.667006	5.327232	-0.017966	2.317689
91.162289	1705.739464	5.332237	-0.018003	2.322626
91.473219	1713.806428	5.337242	-0.018066	2.327561
91.682237	1721.896382	5.342246	-0.018110	2.332491
92.031059	1729.968091	5.347251	-0.018180	2.337411
92.292954	1738.032939	5.352256	-0.018235	2.342309
92.582228	1746.089652	5.357261	-0.018294	2.347195
92.861819	1754.199701	5.362266	-0.018351	2.352101
93.017533	1762.265881	5.367270	-0.018385	2.356961
93.509219	1770.278711	5.372275	-0.018482	2.361806
93.609863	1778.362096	5.377280	-0.018506	2.366651
93.773914	1786.443648	5.382285	-0.018542	2.371491
94.166629	1794.523678	5.387290	-0.018621	2.376338
94.344954	1802.553888	5.392294	-0.018659	2.381128
94.735466	1810.612235	5.397299	-0.018737	2.385943
94.880498	1818.704684	5.402304	-0.018770	2.390748
95.094183	1826.778443	5.407309	-0.018815	2.395538
95.473572	1834.826009	5.412314	-0.018891	2.400316
95.675388	1842.877441	5.417318	-0.018933	2.405072
95.969997	1850.952021	5.422323	-0.018994	2.409840
96.091588	1859.046335	5.427328	-0.019022	2.414597
96.390657	1867.073893	5.432333	-0.019083	2.419319
96.728464	1875.136281	5.437338	-0.019151	2.424055
96.736256	1883.221067	5.442342	-0.019158	2.428770
97.156768	1891.347893	5.447347	-0.019241	2.433531
97.409350	1899.386347	5.452352	-0.019294	2.438219
97.861080	1907.379177	5.457357	-0.019383	2.442886
98.134704	1915.448014	5.462362	-0.019439	2.447575
98.368410	1923.510962	5.467366	-0.019488	2.452249
98.833641	1931.546359	5.472371	-0.019580	2.456915
98.988968	1939.624053	5.477376	-0.019614	2.461573
99.279950	1947.660783	5.482381	-0.019674	2.466209
99.512031	1955.755418	5.487386	-0.019722	2.470865
99.645692	1963.810833	5.492390	-0.019752	2.475483
99.854054	1971.851957	5.497395	-0.019797	2.480089
100.076320	1979.910479	5.502400	-0.019843	2.484697
100.465206	1987.941071	5.507405	-0.019921	2.489294
100.676128	1996.048068	5.512410	-0.019966	2.493912
100.731099	2004.110171	5.517414	-0.019981	2.498484
101.094767	2012.161863	5.522419	-0.020054	2.503065
101.595018	2020.180767	5.527424	-0.020153	2.507629
101.695550	2028.299891	5.532429	-0.020177	2.512212
101.894832	2036.372058	5.537434	-0.020219	2.516767
102.263025	2044.384714	5.542438	-0.020293	2.521293
102.654049	2052.403505	5.547443	-0.020371	2.525816
102.792199	2060.495530	5.552448	-0.020402	2.530353
103.020992	2068.560381	5.557453	-0.020450	2.534874
103.411502	2076.600371	5.562458	-0.020528	2.539384
103.472626	2084.648294	5.567462	-0.020545	2.543867
103.758569	2092.715616	5.572467	-0.020603	2.548369
103.980901	2100.799832	5.577472	-0.020650	2.552867
104.445224	2108.806807	5.582477	-0.020742	2.557332
104.720912	2116.856475	5.587482	-0.020798	2.561800
105.075835	2124.891946	5.592486	-0.020870	2.566257
105.387565	2132.966359	5.597491	-0.020933	2.570725
105.328907	2141.065596	5.602496	-0.020928	2.575173
105.438252	2149.099593	5.607501	-0.020953	2.579589
105.677504	2157.155354	5.612506	-0.021003	2.584019
105.952259	2165.207784	5.617510	-0.021060	2.588441
106.119017	2173.410459	5.622515	-0.021096	2.592931
106.366031	2181.458321	5.627520	-0.021147	2.597333
106.565206	2189.444989	5.632525	-0.021190	2.601692
106.756758	2197.472304	5.637530	-0.021231	2.606065
106.994456	2205.481840	5.642534	-0.021280	2.610424
107.507868	2213.520296	5.647539	-0.021381	2.614810
107.677677	2221.558532	5.652544	-0.021418	2.619166
107.707718	2229.607878	5.657549	-0.021429	2.623510
108.232772	2237.638092	5.662554	-0.021532	2.627870
108.282001	2245.708759	5.667558	-0.021546	2.632213
108.405997	2253.782120	5.672563	-0.021575	2.636556
108.821738	2261.784283	5.677568	-0.021658	2.640872
108.891804	2269.831469	5.682573	-0.021676	2.645182
109.055181	2277.892374	5.687578	-0.021712	2.649499
109.442779	2285.944921	5.692582	-0.021789	2.653819
110.013104	2293.965593	5.697587	-0.021901	2.658127
109.954576	2302.038792	5.702592	-0.021895	2.662414
110.370372	2310.058910	5.707597	-0.021978	2.666698
110.736578	2318.153054	5.712602	-0.022051	2.671010
110.753444	2326.239166	5.717606	-0.022060	2.675289
110.869624	2334.243964	5.722611	-0.022087	2.679524
111.135267	2342.270653	5.727616	-0.022141	2.683774
111.453700	2350.293754	5.732621	-0.022206	2.688018
111.652869	2358.379201	5.737626	-0.022248	2.692281
111.940409	2366.418710	5.742630	-0.022307	2.696519
112.198698	2374.447133	5.747635	-0.022361	2.700742
112.608614	2382.477825	5.752640	-0.022442	2.704969
112.546848	2390.552189	5.757645	-0.022436	2.709183
112.880719	2398.636644	5.762650	-0.022504	2.713420
113.006991	2406.662156	5.767654	-0.022532	2.717607
113.143553	2414.715725	5.772659	-0.022563	2.721802
113.239007	2422.774067	5.777664	-0.022586	2.725992
113.578485	2430.794733	5.782669	-0.022655	2.730170
113.763232	2438.876457	5.787674	-0.022694	2.734364
113.950221	2446.905134	5.792678	-0.022734	2.738524
114.102039	2454.941214	5.797683	-0.022768	2.742679
114.392056	2462.991435	5.802688	-0.022827	2.746844
114.621774	2471.072705	5.807693	-0.022875	2.751014
115.035337	2479.176962	5.812698	-0.022958	2.755202
115.166883	2487.147836	5.817702	-0.022988	2.759297
115.413510	2495.184850	5.822707	-0.023039	2.763427
115.640030	2503.214394	5.827712	-0.023086	2.767546
115.830085	2511.261527	5.832717	-0.023127	2.771666
115.954401	2519.333332	5.837722	-0.023155	2.775788
116.023233	2527.340205	5.842726	-0.023173	2.779867
116.412706	2535.358430	5.847731	-0.023251	2.783965
116.630098	2543.417323	5.852736	-0.023297	2.788068
116.871643	2551.450269	5.857741	-0.023347	2.792153
117.242628	2559.499883	5.862746	-0.023422	2.796248
117.372170	2567.526987	5.867750	-0.023451	2.800311
117.452588	2575.554782	5.872755	-0.023471	2.804366
117.867712	2583.591011	5.877760	-0.023554	2.808438
118.222638	2591.636758	5.882765	-0.023625	2.812506
118.477381	2599.720175	5.887770	-0.023678	2.816581
118.518687	2607.750860	5.892774	-0.023691	2.820612
118.764609	2615.768385	5.897779	-0.023742	2.824642
118.853689	2623.854786	5.902784	-0.023764	2.828691
119.122843	2631.896626	5.907789	-0.023820	2.832723
119.520140	2639.951145	5.912794	-0.023899	2.836763
119.733682	2647.946050	5.917798	-0.023944	2.840756
119.824000	2655.982025	5.922803	-0.023966	2.844758
120.057558	2664.028867	5.927808	-0.024015	2.848767
120.087451	2672.102033	5.932813	-0.024026	2.852772
120.434082	2680.141333	5.937818	-0.024096	2.856773
120.420958	2688.180224	5.942822	-0.024098	2.860748
120.959246	2696.158743	5.947827	-0.024204	2.864717
121.244510	2704.227109	5.952832	-0.024262	2.868712
121.246539	2712.304396	5.957837	-0.024268	2.872690
121.409399	2720.355820	5.962842	-0.024304	2.876658
121.518789	2728.391990	5.967846	-0.024329	2.880611
121.654958	2736.392958	5.972851	-0.024360	2.884542
121.757826	2744.447543	5.977856	-0.024384	2.888492
122.043181	2752.489734	5.982861	-0.024443	2.892441
122.324907	2760.532606	5.987866	-0.024501	2.896384
122.503467	2768.574330	5.992870	-0.024539	2.900316
122.577168	2776.608521	5.997875	-0.024558	2.904233
122.929703	2784.656220	6.002880	-0.024629	2.908167
122.958533	2792.741043	6.007885	-0.024640	2.912095
123.226573	2800.824014	6.012890	-0.024695	2.916031
123.567285	2808.784320	6.017894	-0.024764	2.919905
123.635474	2816.806575	6.022899	-0.024782	2.923790
123.852553	2824.834888	6.027904	-0.024827	2.927680
124.132382	2832.872977	6.032909	-0.024885	2.931573
124.468111	2840.932021	6.037914	-0.024953	2.935474
124.639262	2848.930945	6.042918	-0.024990	2.939332
124.804796	2856.959290	6.047923	-0.025026	2.943199
125.005372	2864.998394	6.052928	-0.025069	2.947068
125.153203	2873.058449	6.057933	-0.025101	2.950939
125.541754	2881.104464	6.062938	-0.025179	2.954811
125.790720	2889.097885	6.067942	-0.025231	2.958645
126.006840	2897.145920	6.072947	-0.025276	2.962498
126.044134	2905.185121	6.077952	-0.025288	2.966333
126.393089	2913.222964	6.082957	-0.025359	2.970179
126.532461	2921.319481	6.087962	-0.025390	2.974036
126.606320	2929.357295	6.092966	-0.025409	2.977858
126.809165	2937.376569	6.097971	-0.025452	2.981672
127.408510	2945.354760	6.102976	-0.025569	2.985482
127.416243	2953.422872	6.107981	-0.025576	2.989299
127.658828	2961.518038	6.112986	-0.025626	2.993136
127.815821	2969.531509	6.117990	-0.025661	2.996926
128.077080	2977.553468	6.122995	-0.025715	3.000720
128.273825	2985.556693	6.128000	-0.025757	3.004497
128.355049	2993.604862	6.133005	-0.025777	3.008284
128.737719	3001.635520	6.138010	-0.025854	3.012074
128.611199	3009.711287	6.143014	-0.025835	3.015855
129.038496	3017.697755	6.148019	-0.025920	3.019616
129.256026	3025.735714	6.153024	-0.025966	3.023386
129.187169	3033.792319	6.158029	-0.025958	3.027147
129.449525	3041.852530	6.163034	-0.026013	3.030920
129.907427	3049.856342	6.168038	-0.026103	3.034672
130.003178	3057.893124	6.173043	-0.026126	3.038418
129.989211	3065.955948	6.178048	-0.026129	3.042165
130.139528	3073.953189	6.183053	-0.026162	3.045885
130.397703	3081.999014	6.188058	-0.026216	3.049628
130.509861	3090.063835	6.193062	-0.026242	3.053369
130.671943	3098.094309	6.198067	-0.026277	3.057091
131.032907	3106.095319	6.203072	-0.026350	3.060805
131.322101	3114.092603	6.208077	-0.026409	3.064509
131.494574	3122.192989	6.213082	-0.026446	3.068250
131.814074	3130.236780	6.218086	-0.026511	3.071968
131.923955	3138.323385	6.223091	-0.026537	3.075691
131.974982	3146.308824	6.228096	-0.026552	3.079360
132.148006	3154.311876	6.233101	-0.026589	3.083039
132.423770	3162.358505	6.238106	-0.026646	3.086738
132.601258	3170.351130	6.243110	-0.026684	3.090403
132.597131	3178.420875	6.248115	-0.026689	3.094091
132.767441	3186.473112	6.253120	-0.026726	3.097774
132.831580	3194.492249	6.258125	-0.026743	3.101433
132.941666	3202.520405	6.263130	-0.026769	3.105094
133.137336	3210.542664	6.268134	-0.026811	3.108752
133.410152	3218.597026	6.273139	-0.026867	3.112423
133.655423	3226.654843	6.278144	-0.026918	3.116091
133.855625	3234.617177	6.283149	-0.026960	3.119708
134.052505	3242.675449	6.288154	-0.027002	3.123365
134.038007	3250.691681	6.293158	-0.027005	3.126989
134.363197	3258.723035	6.298163	-0.027071	3.130631
134.568622	3266.787509	6.303168	-0.027114	3.134278
134.654146	3274.797040	6.308173	-0.027135	3.137891
134.928506	3282.841011	6.313178	-0.027192	3.141523
134.902543	3290.865539	6.318182	-0.027192	3.145130
135.263794	3298.874564	6.323187	-0.027265	3.148742
135.509573	3306.970429	6.328192	-0.027316	3.152383
135.474970	3314.997151	6.333197	-0.027315	3.155978
136.147977	3322.958534	6.338202	-0.027445	3.159570
136.008317	3330.997103	6.343206	-0.027425	3.163157
136.112883	3339.056734	6.348211	-0.027449	3.166759
136.467031	3347.085338	6.353216	-0.027521	3.170355
136.492895	3355.119181	6.358221	-0.027531	3.173935
136.684255	3363.156694	6.363226	-0.027572	3.177519
136.903709	3371.183814	6.368230	-0.027618	3.181096
137.397180	3379.171262	6.373235	-0.027715	3.184663
137.432442	3387.248448	6.378240	-0.027727	3.188246
137.391727	3395.318736	6.383245	-0.027725	3.191819
137.804223	3403.342102	6.388250	-0.027807	3.195386
138.315383	3411.324255	6.393254	-0.027907	3.198935
138.222909	3419.380676	6.398259	-0.027895	3.202488
138.549016	3427.415520	6.403264	-0.027961	3.206044
138.616550	3435.437826	6.408269	-0.027979	3.209580
138.777949	3443.509855	6.413274	-0.028014	3.213139
139.047667	3451.513897	6.418278	-0.028070	3.216667
139.293215	3459.529853	6.423283	-0.028121	3.220197
139.383283	3467.573597	6.428288	-0.028143	3.223728
139.572554	3475.582691	6.433293	-0.028184	3.227244
139.737273	3483.634325	6.438298	-0.028219	3.230773
139.893387	3491.734250	6.443302	-0.028254	3.234320
139.930235	3499.736196	6.448307	-0.028266	3.237815
140.109917	3507.734263	6.453312	-0.028305	3.241310
140.213209	3515.708703	6.458317	-0.028329	3.244789
140.677565	3523.735882	6.463322	-0.028421	3.248300
140.877694	3531.775533	6.468326	-0.028464	3.251803
141.170068	3539.814742	6.473331	-0.028523	3.255306
141.239306	3547.844380	6.478336	-0.028541	3.258792
141.400059	3555.857682	6.483341	-0.028577	3.262270
141.781414	3563.904899	6.488346	-0.028653	3.265768
141.955661	3571.921333	6.493350	-0.028691	3.269241
142.023549	3579.992237	6.498355	-0.028709	3.272730
142.372998	3588.030986	6.503360	-0.028779	3.276212
142.380858	3596.002916	6.508365	-0.028786	3.279648
142.458533	3604.073393	6.513370	-0.028806	3.283125
142.678960	3612.084375	6.518374	-0.028852	3.286579
143.072352	3620.098482	6.523379	-0.028930	3.290038
143.513671	3628.150390	6.528384	-0.029018	3.293510
143.358944	3636.204774	6.533389	-0.028994	3.296957
143.527714	3644.225415	6.538394	-0.029031	3.300399
143.661977	3652.221092	6.543398	-0.029061	3.303824
143.981440	3660.226896	6.548403	-0.029126	3.307258
144.100333	3668.294882	6.553408	-0.029154	3.310707
144.286131	3676.341966	6.558413	-0.029194	3.314146
144.532787	3684.355453	6.563418	-0.029245	3.317569
144.819082	3692.361362	6.568422	-0.029303	3.320987
145.032595	3700.360776	6.573427	-0.029348	3.324396
145.321556	3708.405998	6.578432	-0.029407	3.327824
145.252404	3716.475649	6.583437	-0.029400	3.331245
145.490421	3724.532551	6.588442	-0.029450	3.334668
145.444059	3732.531973	6.593446	-0.029446	3.338053
145.715983	3740.553090	6.598451	-0.029502	3.341456
146.064586	3748.556625	6.603456	-0.029572	3.344851
146.076522	3756.591783	6.608461	-0.029580	3.348243
146.155157	3764.675991	6.613466	-0.029600	3.351654
146.445384	3772.681225	6.618470	-0.029659	3.355037
147.100283	3780.625370	6.623475	-0.029786	3.358404
147.563706	3788.683450	6.628480	-0.029878	3.361808
147.584055	3796.713594	6.633485	-0.029887	3.365181
147.796657	3804.756187	6.638490	-0.029932	3.368563
148.117579	3812.801438	6.643494	-0.029997	3.371946
148.280806	3820.841520	6.648499	-0.030033	3.375318
148.381612	3828.852472	6.653504	-0.030057	3.378673
148.482412	3836.880410	6.658509	-0.030081	3.382031
148.845123	3844.917394	6.663514	-0.030154	3.385398
148.905585	3852.950651	6.668518	-0.030170	3.388750
149.161379	3861.033162	6.673523	-0.030223	3.392126
149.446026	3869.101914	6.678528	-0.030281	3.395494
149.336508	3877.061643	6.683533	-0.030266	3.398800
149.537983	3885.060941	6.688538	-0.030309	3.402130
149.922974	3893.064892	6.693542	-0.030386	3.405464
149.768424	3901.090948	6.698547	-0.030363	3.408786
150.079539	3909.142617	6.703552	-0.030426	3.412131
150.245017	3917.157045	6.708557	-0.030462	3.415453
150.828402	3925.155354	6.713562	-0.030576	3.418779
150.731511	3933.201256	6.718566	-0.030563	3.422098
150.936777	3941.195212	6.723571	-0.030606	3.425402
151.475520	3949.212033	6.728576	-0.030712	3.428724
151.362681	3957.312305	6.733581	-0.030696	3.432056
151.618394	3965.343177	6.738586	-0.030749	3.435367
151.995990	3973.333975	6.743590	-0.030825	3.438664
152.083967	3981.353914	6.748595	-0.030847	3.441959
152.100485	3989.393482	6.753600	-0.030855	3.445257
152.168466	3997.422877	6.758605	-0.030873	3.448549
152.363734	4005.455039	6.763610	-0.030915	3.451843
152.575477	4013.503574	6.768614	-0.030959	3.455142
152.668714	4021.491455	6.773619	-0.030982	3.458408
153.045820	4029.543751	6.778624	-0.031057	3.461707
153.149405	4037.543075	6.783629	-0.031082	3.464972
153.411944	4045.584845	6.788634	-0.031136	3.468257
153.591598	4053.647109	6.793638	-0.031175	3.471544
153.679948	4061.691328	6.798643	-0.031197	3.474818
153.971015	4069.684826	6.803648	-0.031256	3.478075
154.052721	4077.670185	6.808653	-0.031277	3.481318
154.359717	4085.682245	6.813658	-0.031339	3.484576
154.509705	4093.695029	6.818662	-0.031372	3.487827
154.292237	4101.774299	6.823667	-0.031337	3.491090
154.620497	4109.788960	6.828672	-0.031404	3.494341
154.919481	4117.766362	6.833677	-0.031464	3.497573
154.994222	4125.847698	6.838682	-0.031484	3.500836
155.197595	4133.821266	6.843686	-0.031527	3.504058
155.253439	4141.871085	6.848691	-0.031543	3.507302
155.476572	4149.917787	6.853696	-0.031589	3.510547
155.708874	4157.937933	6.858701	-0.031638	3.513779
155.976647	4165.973736	6.863706	-0.031693	3.517016
156.232275	4173.954183	6.868710	-0.031746	3.520226
156.233063	4181.977902	6.873715	-0.031751	3.523444
156.455643	4190.055187	6.878720	-0.031798	3.526686
156.590579	4198.071769	6.883725	-0.031829	3.529899
156.520180	4206.123815	6.888730	-0.031821	3.533116
156.732358	4214.160206	6.893734	-0.031866	3.536333
156.898392	4222.135511	6.898739	-0.031902	3.539521
157.124213	4230.166062	6.903744	-0.031949	3.542730
157.198719	4238.176180	6.908749	-0.031968	3.545924
157.460665	4246.237575	6.913754	-0.032022	3.549140
157.843347	4254.328800	6.918758	-0.032099	3.552370
157.826652	4262.385031	6.923763	-0.032101	3.555570
158.198668	4270.338561	6.928768	-0.032176	3.558738
158.160225	4278.332170	6.933773	-0.032174	3.561907
158.577301	4286.319675	6.938778	-0.032257	3.565084
158.736274	4294.347752	6.943782	-0.032292	3.568267
158.908104	4302.388447	6.948787	-0.032329	3.571453
159.046886	4310.436462	6.953792	-0.032360	3.574637
159.426786	4318.424231	6.958797	-0.032436	3.577802
159.750868	4326.487463	6.963802	-0.032502	3.580992
159.813364	4334.455839	6.968806	-0.032519	3.584134
159.910505	4342.492182	6.973811	-0.032542	3.587302
160.143448	4350.546483	6.978816	-0.032591	3.590477
160.268729	4358.563360	6.983821	-0.032619	3.593632
160.488695	4366.609156	6.988826	-0.032666	3.596798
160.512752	4374.579111	6.993830	-0.032675	3.599926
160.756698	4382.584873	6.998835	-0.032726	3.603071
160.952167	4390.661019	7.003840	-0.032768	3.606240
160.826740	4398.629961	7.008845	-0.032750	3.609355
161.156506	4406.708379	7.013850	-0.032816	3.612523
161.325165	4414.727114	7.018854	-0.032853	3.615660
161.497061	4422.723061	7.023859	-0.032890	3.618786
161.600002	4430.794137	7.028864	-0.032915	3.621936
161.830865	4438.761498	7.033869	-0.032963	3.625047
162.084473	4446.813646	7.038874	-0.033016	3.628189
162.085127	4454.872110	7.043878	-0.033021	3.631323
162.521888	4462.890264	7.048883	-0.033108	3.634451
162.827514	4470.949581	7.053888	-0.033170	3.637589
162.731642	4478.944006	7.058893	-0.033157	3.640688
163.105688	4486.931252	7.063898	-0.033232	3.643794
163.255791	4494.963507	7.068902	-0.033265	3.646909
163.343746	4502.963390	7.073907	-0.033287	3.650007
163.425479	4511.056981	7.078912	-0.033308	3.653138
163.458793	4519.058186	7.083917	-0.033319	3.656230
163.776486	4527.030618	7.088922	-0.033383	3.659315
163.784332	4535.122506	7.093926	-0.033390	3.662436
163.920442	4543.114532	7.098931	-0.033421	3.665519
164.292146	4551.142055	7.103936	-0.033495	3.668619
164.094178	4559.193002	7.108941	-0.033464	3.671711
164.611396	4567.210730	7.113946	-0.033565	3.674806
164.801519	4575.178473	7.118950	-0.033606	3.677870
164.876212	4583.198922	7.123955	-0.033625	3.680950
165.150211	4591.211224	7.128960	-0.033682	3.684028
165.394686	4599.238026	7.133965	-0.033732	3.687109
165.692666	4607.269746	7.138970	-0.033793	3.690190
165.573326	4615.356290	7.143974	-0.033776	3.693280
165.691096	4623.359563	7.148979	-0.033803	3.696340
166.096511	4631.344105	7.153984	-0.033884	3.699399
166.250007	4639.346194	7.158989	-0.033918	3.702455
166.477761	4647.374710	7.163994	-0.033966	3.705520
166.550202	4655.413523	7.168998	-0.033985	3.708583
166.544683	4663.495271	7.174003	-0.033989	3.711658
166.830070	4671.596136	7.179008	-0.034047	3.714745
166.949554	4679.540253	7.184013	-0.034075	3.717765
167.340508	4687.543391	7.189018	-0.034153	3.720812
168.283993	4695.442921	7.194022	-0.034334	3.723831
168.815860	4703.474490	7.199027	-0.034438	3.726887
169.174346	4711.543735	7.204032	-0.034510	3.729951
169.291502	4719.576478	7.209037	-0.034537	3.732992
169.426512	4727.646929	7.214042	-0.034568	3.736046
169.753956	4735.602744	7.219046	-0.034634	3.739058
169.881891	4743.624852	7.224051	-0.034663	3.742089
170.350311	4751.658684	7.229056	-0.034756	3.745129
170.454317	4759.672294	7.234061	-0.034780	3.748150
170.719155	4767.734673	7.239066	-0.034835	3.751191
170.892145	4775.762092	7.244070	-0.034872	3.754215
170.829908	4783.802321	7.249075	-0.034866	3.757235
171.110630	4791.813690	7.254080	-0.034924	3.760250
171.076094	4799.802739	7.259085	-0.034922	3.763247
171.183556	4807.906899	7.264090	-0.034948	3.766288
171.308171	4815.870712	7.269094	-0.034976	3.769274
171.449927	4823.914952	7.274099	-0.035008	3.772288
171.657475	4831.949173	7.279104	-0.035052	3.775298
171.853913	4839.942938	7.284109	-0.035094	3.778289
172.089745	4848.002649	7.289114	-0.035143	3.781304
172.136732	4855.989862	7.294118	-0.035157	3.784286
172.175408	4864.038351	7.299123	-0.035170	3.787287
172.394109	4872.018769	7.304128	-0.035216	3.790265
172.424068	4880.114144	7.309133	-0.035226	3.793279
172.510531	4888.162238	7.314138	-0.035248	3.796274
172.767429	4896.116720	7.319142	-0.035301	3.799236
172.827927	4904.090799	7.324147	-0.035317	3.802198
172.893709	4912.112064	7.329152	-0.035335	3.805176
173.016569	4920.132090	7.334157	-0.035363	3.808152
173.324748	4928.199050	7.339162	-0.035426	3.811148
173.315899	4936.229367	7.344166	-0.035429	3.814120
173.435884	4944.239899	7.349171	-0.035457	3.817086
173.820966	4952.232937	7.354176	-0.035534	3.820048
174.091569	4960.223730	7.359181	-0.035590	3.823005
174.014065	4968.269608	7.364186	-0.035581	3.825972
174.299694	4976.282282	7.369190	-0.035639	3.828933
174.479895	4984.319171	7.374195	-0.035678	3.831898
174.545160	4992.379935	7.379200	-0.035695	3.834867
174.769801	5000.347107	7.384205	-0.035742	3.837803
175.079612	5008.370901	7.389210	-0.035805	3.840759
175.178044	5016.349141	7.394214	-0.035829	3.843691
175.307242	5024.373495	7.399219	-0.035858	3.846639
175.601911	5032.419516	7.404224	-0.035919	3.849596
175.738262	5040.488346	7.409229	-0.035949	3.852555
175.763250	5048.529541	7.414234	-0.035959	3.855500
176.014008	5056.490153	7.419238	-0.036011	3.858418
176.004748	5064.540430	7.424243	-0.036015	3.861361
176.235428	5072.545205	7.429248	-0.036063	3.864290
176.242278	5080.592364	7.434253	-0.036070	3.867228
176.585087	5088.638463	7.439258	-0.036139	3.870170
176.855515	5096.825015	7.444262	-0.036194	3.873159
176.801602	5104.848637	7.449267	-0.036190	3.876081
177.233583	5112.773134	7.454272	-0.036275	3.878973
177.294301	5120.755469	7.459277	-0.036292	3.881877
177.473276	5128.682476	7.464282	-0.036330	3.884761
177.545252	5136.782866	7.469286	-0.036349	3.887704
177.877655	5144.751637	7.474291	-0.036416	3.890602
178.013659	5152.796339	7.479296	-0.036447	3.893521
178.263356	5160.831662	7.484301	-0.036499	3.896437
178.505626	5168.792416	7.489306	-0.036549	3.899324
178.483837	5176.855893	7.494310	-0.036550	3.902241
178.667964	5184.815295	7.499315	-0.036590	3.905121
178.896613	5192.917551	7.504320	-0.036638	3.908052
179.018638	5200.887881	7.509325	-0.036666	3.910931
179.206643	5208.948197	7.514330	-0.036706	3.913842
179.284394	5216.989073	7.519334	-0.036726	3.916741
179.596995	5224.938063	7.524339	-0.036789	3.919610
179.651824	5232.971260	7.529344	-0.036805	3.922502
179.751543	5240.956024	7.534349	-0.036829	3.925375
179.940472	5248.999533	7.539354	-0.036869	3.928269
180.242994	5257.039853	7.544358	-0.036931	3.931161
180.245566	5265.063004	7.549363	-0.036937	3.934040
180.524219	5273.081705	7.554368	-0.036994	3.936920
180.682608	5281.059226	7.559373	-0.037029	3.939781
180.686264	5289.109625	7.564378	-0.037034	3.942663
180.793606	5297.105797	7.569382	-0.037060	3.945526
181.166784	5305.116569	7.574387	-0.037135	3.948396
181.134554	5313.195200	7.579392	-0.037134	3.951282
181.313263	5321.231796	7.584397	-0.037172	3.954153
181.670173	5329.223615	7.589402	-0.037244	3.957010
181.763648	5337.206983	7.594406	-0.037267	3.959858
181.833564	5345.211310	7.599411	-0.037285	3.962710
182.253176	5353.244981	7.604416	-0.037369	3.965577
182.396664	5361.243438	7.609421	-0.037401	3.968424
182.448127	5369.321519	7.614426	-0.037415	3.971296
182.712044	5377.339980	7.619430	-0.037470	3.974148
182.649873	5385.357755	7.624435	-0.037464	3.976992
183.070436	5393.359377	7.629440	-0.037547	3.979837
183.261695	5401.388248	7.634445	-0.037588	3.982686
183.503345	5409.398553	7.639450	-0.037638	3.985526
183.544197	5417.461979	7.644454	-0.037651	3.988381
183.680075	5425.467627	7.649459	-0.037682	3.991214
184.118718	5433.502173	7.654464	-0.037769	3.994060
184.281861	5441.532311	7.659469	-0.037804	3.996898
184.458529	5449.489727	7.664474	-0.037843	3.999709
184.720577	5457.548130	7.669478	-0.037897	4.002555
184.718063	5465.534872	7.674483	-0.037902	4.005369
185.044194	5473.581570	7.679488	-0.037968	4.008208
184.960966	5481.631232	7.684493	-0.037957	4.011039
185.415793	5489.637580	7.689498	-0.038047	4.013861
185.559991	5497.706282	7.694502	-0.038079	4.016698
185.727847	5505.640057	7.699507	-0.038116	4.019486
185.752579	5513.731725	7.704512	-0.038126	4.022326
186.104165	5521.702507	7.709517	-0.038197	4.025126
186.297120	5529.692185	7.714522	-0.038238	4.027928
186.394083	5537.749683	7.719526	-0.038261	4.030751
186.568370	5545.844332	7.724531	-0.038299	4.033586
186.688677	5553.923866	7.729536	-0.038327	4.036412
186.608821	5561.796054	7.734541	-0.038317	4.039162
186.923592	5569.824833	7.739546	-0.038381	4.041969
187.294777	5577.821124	7.744550	-0.038455	4.044765
187.129659	5585.831550	7.749555	-0.038430	4.047555
187.195814	5593.873521	7.754560	-0.038447	4.050358
187.329868	5601.910168	7.759565	-0.038478	4.053158
187.660954	5609.914563	7.764570	-0.038545	4.055948
187.809268	5617.915168	7.769574	-0.038578	4.058732
187.841732	5625.942321	7.774579	-0.038589	4.061522
188.136752	5633.925494	7.779584	-0.038649	4.064298
188.371599	5641.941031	7.784589	-0.038698	4.067082
188.571425	5649.977109	7.789594	-0.038741	4.069871
188.933314	5658.050953	7.794598	-0.038813	4.072674
188.773805	5666.008228	7.799603	-0.038789	4.075427
189.002189	5674.040027	7.804608	-0.038837	4.078209
189.174945	5682.037194	7.809613	-0.038874	4.080977
189.364582	5690.035581	7.814618	-0.038915	4.083743
189.529965	5698.088376	7.819622	-0.038951	4.086526
189.669021	5706.091665	7.824627	-0.038982	4.089290
189.876972	5714.149346	7.829632	-0.039026	4.092071
190.132710	5722.161792	7.834637	-0.039079	4.094836
190.070330	5730.209391	7.839642	-0.039073	4.097606
190.339626	5738.214168	7.844646	-0.039128	4.100365
190.265215	5746.195937	7.849651	-0.039119	4.103109
190.465008	5754.241567	7.854656	-0.039162	4.105876
190.612747	5762.249235	7.859661	-0.039195	4.108628
190.904561	5770.295087	7.864666	-0.039254	4.111393
191.324044	5778.377174	7.869670	-0.039338	4.114171
191.418113	5786.333166	7.874675	-0.039361	4.116899
191.642575	5794.306928	7.879680	-0.039408	4.119633
191.447970	5802.343653	7.884685	-0.039377	4.122381
191.704445	5810.355275	7.889690	-0.039430	4.125125
191.939453	5818.399631	7.894694	-0.039479	4.127877
191.992706	5826.407663	7.899699	-0.039494	4.130613
192.240132	5834.459703	7.904704	-0.039545	4.133365
192.449127	5842.481077	7.909709	-0.039590	4.136104
192.616471	5850.448900	7.914714	-0.039626	4.138822
193.000654	5858.515103	7.919718	-0.039703	4.141575
192.998106	5866.455689	7.924723	-0.039708	4.144278
193.318035	5874.545162	7.929728	-0.039772	4.147035
193.477964	5882.539246	7.934733	-0.039808	4.149754
193.555545	5890.617827	7.939738	-0.039827	4.152500
193.867060	5898.637531	7.944742	-0.039891	4.155227
193.749221	5906.609419	7.949747	-0.039874	4.157931
194.004458	5914.660162	7.954752	-0.039927	4.160664
194.020957	5922.648928	7.959757	-0.039935	4.163371
194.202107	5930.635449	7.964762	-0.039974	4.166078
194.416863	5938.702699	7.969766	-0.040019	4.168811
194.607108	5946.717990	7.974771	-0.040060	4.171524
194.928459	5954.730496	7.979776	-0.040125	4.174235
195.067992	5962.777525	7.984781	-0.040156	4.176955
195.076757	5970.737971	7.989786	-0.040163	4.179642
195.281804	5978.794299	7.994790	-0.040207	4.182362
195.457979	5986.754075	7.999795	-0.040245	4.185047
195.649339	5994.821448	8.004800	-0.040286	4.187767
195.645770	6002.832740	8.009805	-0.040290	4.190464
195.950549	6010.954387	8.014810	-0.040353	4.193200
196.171261	6018.958765	8.019814	-0.040399	4.195894
196.189081	6026.873518	8.024819	-0.040408	4.198553
196.634757	6034.904424	8.029824	-0.040496	4.201255
196.882598	6042.867791	8.034829	-0.040547	4.203930
197.037601	6050.933287	8.039834	-0.040581	4.206636
197.031372	6058.918655	8.044838	-0.040585	4.209312
197.334398	6066.964860	8.049843	-0.040647	4.212010
197.432282	6074.987175	8.054848	-0.040671	4.214696
197.520317	6083.005619	8.059853	-0.040692	4.217380
197.827155	6090.965616	8.064858	-0.040755	4.220044
197.975485	6098.984143	8.069862	-0.040788	4.222724
197.975191	6107.032843	8.074867	-0.040793	4.225411
198.110911	6115.038652	8.079872	-0.040823	4.228083
198.390002	6123.070659	8.084877	-0.040881	4.230764
198.380045	6131.088214	8.089882	-0.040884	4.233436
198.623619	6139.170062	8.094886	-0.040935	4.236129
198.887922	6147.093278	8.099891	-0.040989	4.238769
198.965930	6155.162101	8.104896	-0.041009	4.241453
199.104239	6163.124425	8.109901	-0.041040	4.244101
199.290192	6171.179757	8.114906	-0.041080	4.246778
199.533841	6179.221704	8.119910	-0.041131	4.249450
199.578238	6187.218828	8.124915	-0.041144	4.252103
199.826527	6195.289749	8.129920	-0.041196	4.254781
200.142980	6203.219775	8.134925	-0.041260	4.257412
200.359297	6211.241515	8.139930	-0.041306	4.260070
200.143173	6219.296117	8.144934	-0.041271	4.262733
200.502219	6227.302436	8.149939	-0.041343	4.265384
200.661276	6235.340016	8.154944	-0.041378	4.268042
200.739263	6243.388609	8.159949	-0.041397	4.270701
200.941820	6251.422897	8.164954	-0.041441	4.273355
201.225738	6259.490440	8.169958	-0.041499	4.276018
201.289979	6267.405890	8.174963	-0.041516	4.278628
201.329919	6275.489871	8.179968	-0.041529	4.281292
201.604923	6283.398386	8.184973	-0.041585	4.283898
201.500173	6291.478054	8.189978	-0.041571	4.286556
201.747037	6299.432305	8.194982	-0.041622	4.289174
202.173810	6307.497264	8.199987	-0.041707	4.291828
202.311885	6315.556476	8.204992	-0.041738	4.294476
202.384115	6323.588090	8.209997	-0.041757	4.297113
202.585466	6331.525374	8.215002	-0.041799	4.299718
202.677808	6339.593082	8.220006	-0.041822	4.302364
202.789980	6347.552848	8.225011	-0.041848	4.304972
203.064017	6355.636684	8.230016	-0.041904	4.307621
203.313991	6363.623110	8.235021	-0.041956	4.310237
203.302385	6371.662630	8.240026	-0.041959	4.312866
203.264299	6379.707673	8.245030	-0.041958	4.315495
203.709896	6387.693904	8.250035	-0.042046	4.318107
203.712426	6395.702914	8.255040	-0.042052	4.320721
203.841241	6403.679466	8.260045	-0.042081	4.323324
204.039872	6411.705298	8.265050	-0.042123	4.325942
204.397870	6419.730621	8.270054	-0.042195	4.328560
204.448253	6427.742794	8.275059	-0.042210	4.331169
204.744312	6435.807244	8.280064	-0.042270	4.333796
205.043647	6443.841114	8.285069	-0.042331	4.336411
205.121420	6451.763651	8.290074	-0.042351	4.338986
205.291729	6459.864900	8.295078	-0.042388	4.341619
205.427716	6467.820836	8.300083	-0.042418	4.344203
205.620626	6475.905515	8.305088	-0.042460	4.346827
205.487310	6483.901740	8.310093	-0.042440	4.349419
205.768500	6491.906733	8.315098	-0.042498	4.352015
206.107297	6500.062031	8.320102	-0.042566	4.354658
205.905237	6507.953473	8.325107	-0.042534	4.357211
206.162427	6515.959087	8.330112	-0.042587	4.359802
206.603726	6524.005558	8.335117	-0.042674	4.362407
206.739573	6531.926684	8.340122	-0.042705	4.364967
206.704567	6539.956405	8.345126	-0.042704	4.367559
206.976188	6547.970516	8.350131	-0.042760	4.370147
207.458965	6556.045539	8.355136	-0.042855	4.372754
207.512906	6564.066752	8.360141	-0.042870	4.375340
207.620222	6572.062666	8.365146	-0.042895	4.377916
208.117392	6580.082390	8.370150	-0.042993	4.380501
208.092862	6588.045656	8.375155	-0.042994	4.383063
208.033714	6596.101610	8.380160	-0.042988	4.385653
208.348453	6604.146932	8.385165	-0.043052	4.388240
208.592065	6612.132261	8.390170	-0.043103	4.390806
208.670125	6620.201129	8.395174	-0.043123	4.393396
208.545463	6628.179950	8.400179	-0.043105	4.395955
208.906846	6636.169745	8.405184	-0.043177	4.398518
208.972702	6644.229737	8.410189	-0.043195	4.401101
209.215271	6652.191119	8.415194	-0.043245	4.403652
209.563385	6660.229655	8.420198	-0.043315	4.406226
209.507618	6668.255165	8.425203	-0.043310	4.408793
209.713404	6676.306556	8.430208	-0.043354	4.411368
210.019676	6684.308367	8.435213	-0.043416	4.413926
210.220634	6692.324417	8.440218	-0.043459	4.416486
210.412617	6700.307176	8.445222	-0.043500	4.419034
210.404894	6708.378941	8.450227	-0.043504	4.421608
210.568085	6716.339189	8.455232	-0.043539	4.424146
210.676550	6724.426461	8.460237	-0.043565	4.426723
210.787514	6732.405647	8.465242	-0.043591	4.429263
211.160739	6740.477947	8.470246	-0.043666	4.431833
211.171027	6748.470882	8.475251	-0.043673	4.434375
211.364636	6756.498270	8.480256	-0.043714	4.436927
211.571785	6764.481997	8.485261	-0.043758	4.439464
211.694489	6772.527611	8.490266	-0.043786	4.442018
211.774345	6780.465284	8.495270	-0.043806	4.444536
211.782758	6788.552249	8.500275	-0.043813	4.447101
212.197087	6796.535109	8.505280	-0.043896	4.449632
212.427910	6804.581255	8.510285	-0.043944	4.452181
212.261923	6812.563144	8.515290	-0.043918	4.454707
212.703886	6820.644586	8.520294	-0.044006	4.457265
212.851794	6828.585311	8.525299	-0.044039	4.459776
212.919287	6836.611606	8.530304	-0.044057	4.462312
213.188122	6844.613406	8.535309	-0.044112	4.464840
213.479829	6852.674999	8.540314	-0.044171	4.467385
213.590173	6860.696867	8.545318	-0.044197	4.469916
213.508305	6868.709657	8.550323	-0.044187	4.472442
213.676855	6876.733089	8.555328	-0.044224	4.474970
213.742238	6884.756309	8.560333	-0.044241	4.477497
213.754081	6892.709255	8.565338	-0.044249	4.480000
213.954765	6900.751049	8.570343	-0.044292	4.482530
214.102978	6908.739404	8.575347	-0.044324	4.485042
214.389574	6916.801473	8.580352	-0.044383	4.487575
214.512375	6924.812165	8.585357	-0.044411	4.490091
214.609245	6932.828654	8.590362	-0.044435	4.492607
214.812917	6940.847666	8.595367	-0.044478	4.495123
214.799759	6948.840414	8.600371	-0.044481	4.497628
215.176708	6956.844010	8.605376	-0.044556	4.500137
215.368410	6964.854888	8.610381	-0.044597	4.502646
215.537538	6972.855548	8.615386	-0.044634	4.505150
215.805914	6980.913799	8.620391	-0.044689	4.507671
216.118272	6988.928352	8.625395	-0.044753	4.510177
216.133345	6997.013906	8.630400	-0.044761	4.512703
216.324855	7005.049583	8.635405	-0.044802	4.515212
216.519610	7012.966698	8.640410	-0.044843	4.517683
216.482294	7021.005146	8.645415	-0.044842	4.520190
216.501763	7028.972490	8.650419	-0.044850	4.522674
216.799456	7036.955249	8.655424	-0.044911	4.525162
216.998887	7045.033483	8.660429	-0.044954	4.527677
217.045680	7053.000932	8.665434	-0.044968	4.530157
217.255106	7061.075111	8.670439	-0.045012	4.532668
217.438876	7069.076667	8.675443	-0.045051	4.535156
217.709254	7077.094217	8.680448	-0.045107	4.537647
217.807389	7085.101239	8.685453	-0.045130	4.540134
217.977943	7093.091139	8.690458	-0.045168	4.542614
218.010993	7101.130562	8.695463	-0.045179	4.545107
218.185437	7109.124282	8.700467	-0.045217	4.547585
218.373592	7117.145550	8.705472	-0.045257	4.550071
218.660113	7125.214153	8.710477	-0.045316	4.552570
218.654714	7133.228191	8.715482	-0.045320	4.555050
218.971224	7141.276390	8.720487	-0.045384	4.557540
219.088592	7149.192631	8.725491	-0.045411	4.559987
219.091054	7157.251134	8.730496	-0.045417	4.562477
219.119237	7165.236073	8.735501	-0.045428	4.564942
219.181980	7173.295029	8.740506	-0.045445	4.567430
219.574821	7181.316687	8.745511	-0.045523	4.569905
219.571691	7189.363497	8.750515	-0.045528	4.572385
219.848239	7197.339765	8.755520	-0.045585	4.574843
219.732305	7205.399754	8.760525	-0.045568	4.577325
219.895290	7213.329330	8.765530	-0.045604	4.579766
219.886121	7221.372302	8.770535	-0.045607	4.582240
220.102540	7229.372327	8.775539	-0.045653	4.584700
220.578588	7237.431005	8.780544	-0.045747	4.587177
220.490605	7245.461900	8.785549	-0.045736	4.589643
220.681053	7253.501626	8.790554	-0.045777	4.592111
220.956799	7261.549680	8.795559	-0.045833	4.594580
220.868062	7269.541647	8.800563	-0.045822	4.597031
221.149105	7277.476197	8.805568	-0.045880	4.599462
221.505462	7285.532224	8.810573	-0.045951	4.601930
221.575792	7293.459371	8.815578	-0.045970	4.604357
221.701427	7301.595844	8.820583	-0.045998	4.606846
221.951262	7309.539605	8.825587	-0.046050	4.609276
222.104987	7317.584768	8.830592	-0.046084	4.611734
222.093510	7325.621039	8.835597	-0.046087	4.614189
222.290222	7333.622719	8.840602	-0.046129	4.616632
222.690817	7341.636945	8.845607	-0.046209	4.619078
222.692510	7349.660555	8.850611	-0.046215	4.621525
222.641379	7357.611559	8.855616	-0.046210	4.623948
223.042986	7365.673668	8.860621	-0.046290	4.626404
223.119633	7373.689664	8.865626	-0.046310	4.628845
223.209614	7381.728413	8.870631	-0.046332	4.631292
223.356437	7389.769479	8.875635	-0.046365	4.633737
223.532088	7397.807713	8.880640	-0.046403	4.636181
223.917429	7405.719071	8.885645	-0.046480	4.638585
223.956971	7413.774902	8.890650	-0.046492	4.641031
224.361973	7421.757589	8.895655	-0.046573	4.643454
224.337612	7429.807439	8.900659	-0.046574	4.645896
224.422829	7437.800001	8.905664	-0.046595	4.648319
224.542275	7445.848391	8.910669	-0.046622	4.650758
224.782804	7453.831302	8.915674	-0.046672	4.653176
225.008913	7461.914357	8.920679	-0.046720	4.655622
225.255013	7469.869714	8.925683	-0.046771	4.658029
225.365250	7477.877351	8.930688	-0.046797	4.660450
225.518481	7485.921390	8.935693	-0.046831	4.662882
225.546161	7493.915453	8.940698	-0.046841	4.665296
225.789239	7501.955924	8.945703	-0.046892	4.667724
225.929608	7509.954713	8.950707	-0.046923	4.670137
226.077622	7518.014682	8.955712	-0.046956	4.672568
226.140333	7526.112701	8.960717	-0.046973	4.675009
226.243450	7534.028619	8.965722	-0.046997	4.677394
226.399525	7541.993482	8.970727	-0.047032	4.679792
226.616426	7550.035443	8.975731	-0.047077	4.682213
226.822210	7557.967410	8.980736	-0.047121	4.684599
226.898754	7566.050262	8.985741	-0.047140	4.687029
226.910463	7573.996684	8.990746	-0.047148	4.689417
227.260986	7582.110358	8.995751	-0.047218	4.691853
227.060475	7590.098064	9.000755	-0.047186	4.694251
227.357819	7598.090891	9.005760	-0.047247	4.696649
227.655386	7606.109794	9.010765	-0.047308	4.699053
227.883940	7614.123082	9.015770	-0.047356	4.701455
227.903330	7622.105745	9.020775	-0.047364	4.703846
228.261986	7630.163754	9.025779	-0.047436	4.706258
228.602127	7638.182083	9.030784	-0.047505	4.708657
228.564661	7646.218485	9.035789	-0.047503	4.711061
228.778088	7654.227508	9.040794	-0.047548	4.713455
228.924687	7662.272559	9.045799	-0.047581	4.715859
228.842672	7670.222673	9.050803	-0.047571	4.718233
228.943018	7678.271397	9.055808	-0.047595	4.720636
229.194496	7686.284739	9.060813	-0.047647	4.723026
229.255139	7694.284869	9.065818	-0.047664	4.725412
229.563007	7702.332144	9.070823	-0.047726	4.727809
229.578727	7710.352659	9.075827	-0.047735	4.730198
229.765813	7718.379891	9.080832	-0.047775	4.732588
229.986883	7726.435718	9.085837	-0.047821	4.734985
230.038080	7734.410081	9.090842	-0.047836	4.737357
230.221613	7742.457003	9.095847	-0.047875	4.739748
230.671660	7750.459267	9.100851	-0.047964	4.742125
230.503982	7758.355267	9.105856	-0.047938	4.744470
230.680872	7766.451249	9.110861	-0.047977	4.746873
230.966510	7774.465211	9.115866	-0.048035	4.749250
230.957385	7782.510636	9.120871	-0.048039	4.751636
231.130794	7790.575829	9.125875	-0.048076	4.754026
231.358160	7798.539295	9.130880	-0.048124	4.756384
231.607689	7806.570343	9.135885	-0.048176	4.758761
231.623614	7814.509928	9.140890	-0.048184	4.761111
231.997847	7822.533709	9.145895	-0.048259	4.763483
232.017732	7830.561596	9.150899	-0.048268	4.765856
232.142485	7838.553570	9.155904	-0.048296	4.768217
232.279524	7846.613153	9.160909	-0.048327	4.770597
232.487307	7854.602608	9.165914	-0.048371	4.772955
232.499580	7862.627460	9.170919	-0.048379	4.775323
232.691247	7870.625818	9.175923	-0.048420	4.777681
233.181533	7878.666059	9.180928	-0.048516	4.780049
233.238190	7886.697246	9.185933	-0.048532	4.782415
233.143039	7894.605236	9.190938	-0.048520	4.784744
233.470103	7902.729775	9.195943	-0.048586	4.787134
233.472592	7910.683055	9.200947	-0.048592	4.789473
233.642383	7918.733946	9.205952	-0.048629	4.791840
233.919521	7926.743679	9.210957	-0.048685	4.794192
233.910763	7934.804322	9.215962	-0.048689	4.796560
234.130406	7942.721289	9.220967	-0.048735	4.798883
234.073380	7950.799797	9.225971	-0.048730	4.801254
234.332135	7958.799767	9.230976	-0.048783	4.803600
234.468708	7966.797616	9.235981	-0.048814	4.805944
234.541411	7974.810160	9.240986	-0.048833	4.808291
234.737645	7982.836064	9.245991	-0.048875	4.810641
234.877462	7990.326348	9.250995	-0.048906	4.812833
234.889710	7995.057287	9.256000	-0.048911	4.814217

235.111477	7997.674346	9.261005	-0.048954	4.814981
235.219318	7998.933364	9.266010	-0.048975	4.815349
235.484687	7999.399820	9.271015	-0.049025	4.815484
235.410092	8000.491646	9.276019	-0.049012	4.815804
235.500793	8000.510198	9.281024	-0.049029	4.815809
235.571932	8000.511355	9.286029	-0.049042	4.815809
235.588820	8000.488149	9.291034	-0.049045	4.815802
235.829067	8000.519797	9.296039	-0.049090	4.815810
235.713680	8000.489113	9.301043	-0.049069	4.815802
235.723410	8000.505288	9.306048	-0.049071	4.815807
235.820982	8000.521817	9.311053	-0.049089	4.815811
235.885586	8000.496181	9.316058	-0.049101	4.815803
236.069675	8000.547202	9.321063	-0.049135	4.815817
235.775636	8000.510424	9.326067	-0.049081	4.815808
235.854522	8000.521313	9.331072	-0.049095	4.815811
236.252919	8000.525633	9.336077	-0.049170	4.815810
236.116197	8000.497805	9.341082	-0.049144	4.815803
236.148127	8000.511137	9.346087	-0.049150	4.815806
236.281475	8000.493019	9.351091	-0.049175	4.815800
236.241899	8000.516936	9.356096	-0.049168	4.815808
236.388971	8000.522524	9.361101	-0.049195	4.815808
236.480248	8000.503725	9.366106	-0.049212	4.815803
236.327980	8000.531155	9.371111	-0.049184	4.815811
236.349105	8000.502680	9.376115	-0.049188	4.815803
236.625309	8000.523169	9.381120	-0.049239	4.815808
236.719860	8000.444645	9.386125	-0.049257	4.815784
236.578894	8000.491472	9.391130	-0.049231	4.815798
236.627968	8000.546713	9.396135	-0.049240	4.815814
236.464020	8000.542996	9.401139	-0.049210	4.815814
236.466964	8000.551589	9.406144	-0.049210	4.815817
236.468895	8000.528141	9.411149	-0.049211	4.815810
236.393406	8000.505575	9.416154	-0.049197	4.815803
236.775160	8000.444510	9.421159	-0.049268	4.815784
236.697598	8000.527590	9.426163	-0.049253	4.815808
236.666828	8000.543109	9.431168	-0.049248	4.815813
236.870590	8000.534671	9.436173	-0.049286	4.815810
236.722914	8000.522678	9.441178	-0.049258	4.815807
236.719926	8000.459654	9.446183	-0.049258	4.815789
236.997515	8000.541013	9.451187	-0.049310	4.815811
236.766885	8000.546891	9.456192	-0.049267	4.815814
236.981238	8000.521545	9.461197	-0.049307	4.815805
236.789989	8000.510981	9.466202	-0.049271	4.815803
236.987610	8000.550481	9.471207	-0.049308	4.815814
236.585866	8000.515159	9.476211	-0.049233	4.815805
236.691330	8000.522209	9.481216	-0.049253	4.815807
236.790421	8000.531291	9.486221	-0.049271	4.815809
236.664847	8000.536735	9.491226	-0.049248	4.815811
236.661695	8000.453427	9.496231	-0.049248	4.815787
236.668659	8000.511188	9.501235	-0.049249	4.815804
236.802147	8000.558189	9.506240	-0.049274	4.815817
236.793804	8000.528170	9.511245	-0.049272	4.815808
236.860448	8000.518579	9.516250	-0.049285	4.815805
236.864984	8000.551750	9.521255	-0.049286	4.815815
236.975230	8000.524719	9.526259	-0.049306	4.815806
236.982086	8000.538712	9.531264	-0.049308	4.815810
237.177439	8000.537611	9.536269	-0.049344	4.815809
237.092755	8000.507423	9.541274	-0.049328	4.815801
237.066535	8000.555041	9.546279	-0.049324	4.815815
236.961147	8000.459401	9.551283	-0.049304	4.815787
237.142459	8000.502906	9.556288	-0.049338	4.815799
237.221244	8000.579979	9.561293	-0.049353	4.815821
236.949182	8000.552094	9.566298	-0.049302	4.815814
237.137891	8000.472959	9.571303	-0.049337	4.815790
237.069367	8000.533768	9.576307	-0.049324	4.815808
237.025689	8000.539471	9.581312	-0.049316	4.815810
237.093628	8000.526699	9.586317	-0.049329	4.815806
237.039804	8000.497011	9.591322	-0.049319	4.815798
237.007795	8000.544535	9.596327	-0.049313	4.815812
237.081703	8000.525455	9.601331	-0.049327	4.815806
237.216694	8000.524444	9.606336	-0.049352	4.815805
237.330613	8000.541239	9.611341	-0.049374	4.815809
237.175025	8000.521644	9.616346	-0.049345	4.815804
237.382238	8000.552761	9.621351	-0.049383	4.815813
237.366433	8000.529025	9.626355	-0.049380	4.815806
237.126678	8000.469638	9.631360	-0.049336	4.815789
237.284039	8000.552253	9.636365	-0.049365	4.815813
237.328505	8000.524157	9.641370	-0.049374	4.815804
237.331645	8000.544495	9.646375	-0.049374	4.815810
237.283550	8000.502089	9.651379	-0.049365	4.815798
237.320663	8000.479211	9.656384	-0.049372	4.815791
237.417976	8000.561922	9.661389	-0.049390	4.815815
237.175089	8000.544116	9.666394	-0.049345	4.815811
237.231027	8000.554634	9.671399	-0.049356	4.815814
237.351726	8000.550189	9.676403	-0.049378	4.815812
237.330633	8000.555191	9.681408	-0.049374	4.815813
237.544380	8000.486068	9.686413	-0.049414	4.815792
237.396401	8000.523174	9.691418	-0.049387	4.815804
237.376113	8000.575158	9.696423	-0.049383	4.815819
237.433980	8000.528063	9.701427	-0.049394	4.815805
237.597886	8000.462403	9.706432	-0.049424	4.815785
237.435854	8000.554792	9.711437	-0.049394	4.815813
237.322750	8000.530548	9.716442	-0.049373	4.815806
237.452267	8000.574283	9.721447	-0.049398	4.815818
237.555373	8000.484154	9.726451	-0.049417	4.815792
237.515202	8000.573178	9.731456	-0.049409	4.815818
237.360785	8000.473540	9.736461	-0.049381	4.815789
237.249096	8000.516571	9.741466	-0.049360	4.815803
237.260349	8000.539176	9.746471	-0.049362	4.815809
237.245143	8000.553880	9.751475	-0.049359	4.815813
237.476464	8000.553362	9.756480	-0.049402	4.815812
237.625467	8000.463976	9.761485	-0.049430	4.815785
237.401993	8000.551099	9.766490	-0.049389	4.815812
237.533160	8000.572444	9.771495	-0.049413	4.815818
237.556377	8000.545070	9.776499	-0.049418	4.815809
237.412914	8000.459487	9.781504	-0.049391	4.815785
237.234619	8000.572961	9.786509	-0.049358	4.815819
237.301001	8000.555894	9.791514	-0.049370	4.815814
237.277718	8000.497878	9.796519	-0.049366	4.815797
237.219550	8000.549248	9.801523	-0.049355	4.815812
237.396149	8000.546776	9.806528	-0.049388	4.815811
237.433389	8000.457715	9.811533	-0.049395	4.815784
237.331232	8000.531858	9.816538	-0.049376	4.815807
237.364513	8000.533470	9.821543	-0.049382	4.815807
237.496368	8000.530273	9.826547	-0.049407	4.815805
237.599909	8000.533023	9.831552	-0.049426	4.815806
237.575601	8000.550782	9.836557	-0.049422	4.815811
237.536234	8000.537340	9.841562	-0.049415	4.815807
237.472350	8000.552323	9.846567	-0.049403	4.815812
237.559053	8000.440578	9.851571	-0.049419	4.815779
237.486054	8000.567501	9.856576	-0.049405	4.815816
237.684453	8000.564315	9.861581	-0.049442	4.815814
237.696368	8000.539960	9.866586	-0.049445	4.815807
237.496497	8000.567686	9.871591	-0.049408	4.815816
237.582766	8000.467676	9.876595	-0.049424	4.815787
237.590550	8000.538262	9.881600	-0.049425	4.815807
237.665711	8000.542687	9.886605	-0.049439	4.815808
237.498990	8000.530385	9.891610	-0.049408	4.815805
237.538902	8000.568399	9.896615	-0.049416	4.815816
237.505826	8000.539046	9.901619	-0.049410	4.815808
237.567680	8000.528311	9.906624	-0.049421	4.815804
237.802489	8000.549200	9.911629	-0.049465	4.815809
237.545269	8000.532228	9.916634	-0.049417	4.815806
237.639614	8000.489994	9.921639	-0.049435	4.815793
237.629763	8000.479165	9.926643	-0.049433	4.815790
237.543838	8000.556773	9.931648	-0.049417	4.815813
237.744000	8000.558954	9.936653	-0.049454	4.815813
237.569981	8000.535857	9.941658	-0.049422	4.815807
237.656886	8000.568228	9.946663	-0.049438	4.815816
237.544751	8000.461802	9.951667	-0.049418	4.815785
237.573463	8000.526322	9.956672	-0.049423	4.815804
237.788673	8000.562906	9.961677	-0.049463	4.815813
237.607805	8000.520484	9.966682	-0.049429	4.815802
237.526632	8000.557604	9.971687	-0.049414	4.815813
237.565511	8000.539024	9.976691	-0.049422	4.815808
237.566199	8000.556121	9.981696	-0.049422	4.815813
237.393288	8000.553325	9.986701	-0.049390	4.815813
237.450516	8000.524368	9.991706	-0.049400	4.815804
237.698708	8000.561486	9.996711	-0.049447	4.815813
237.601581	8000.538568	10.001715	-0.049429	4.815807
237.532810	8000.550269	10.006720	-0.049416	4.815811
237.794182	8000.474445	10.011725	-0.049465	4.815788
237.643396	8000.557408	10.016730	-0.049437	4.815813
237.624890	8000.572059	10.021735	-0.049433	4.815817
237.674996	8000.549391	10.026739	-0.049443	4.815810
237.781376	8000.459314	10.031744	-0.049463	4.815783
237.726296	8000.556637	10.036749	-0.049452	4.815812
237.656761	8000.532031	10.041754	-0.049440	4.815805
237.701302	8000.564783	10.046759	-0.049448	4.815814
237.744156	8000.548403	10.051763	-0.049456	4.815809
237.551335	8000.515394	10.056768	-0.049420	4.815801
237.652615	8000.542660	10.061773	-0.049439	4.815808
237.579776	8000.489178	10.066778	-0.049425	4.815793
237.693028	8000.561473	10.071783	-0.049447	4.815813
237.485653	8000.525027	10.076787	-0.049408	4.815804
237.470514	8000.527989	10.081792	-0.049405	4.815805
237.649191	8000.553306	10.086797	-0.049439	4.815811
237.513970	8000.508421	10.091802	-0.049414	4.815799
237.750684	8000.516531	10.096807	-0.049458	4.815800
237.833492	8000.544565	10.101811	-0.049473	4.815808
237.672560	8000.509938	10.106816	-0.049443	4.815798
237.951743	8000.547559	10.111821	-0.049495	4.815808
237.816207	8000.495196	10.116826	-0.049470	4.815793
237.864352	8000.516264	10.121831	-0.049479	4.815799
238.049073	8000.536342	10.126835	-0.049514	4.815804
237.740062	8000.540948	10.131840	-0.049456	4.815807
237.718969	8000.531004	10.136845	-0.049452	4.815804
237.690481	8000.538021	10.141850	-0.049447	4.815807
237.907469	8000.456141	10.146855	-0.049487	4.815782
237.940091	8000.533535	10.151859	-0.049494	4.815804
237.806093	8000.520694	10.156864	-0.049469	4.815801
238.045794	8000.558743	10.161869	-0.049513	4.815811
237.898159	8000.512589	10.166874	-0.049486	4.815798
238.087071	8000.562625	10.171879	-0.049521	4.815812
237.947011	8000.545416	10.176883	-0.049495	4.815808
237.822856	8000.497507	10.181888	-0.049472	4.815794
237.996694	8000.543029	10.186893	-0.049505	4.815807
237.959681	8000.523219	10.191898	-0.049498	4.815801
238.064329	8000.568688	10.196903	-0.049517	4.815814
238.067139	8000.533511	10.201907	-0.049518	4.815803
238.021159	8000.538109	10.206912	-0.049509	4.815805
238.295170	8000.548959	10.211917	-0.049560	4.815807
237.981095	8000.555618	10.216922	-0.049502	4.815810
237.938435	8000.554932	10.221927	-0.049494	4.815810
238.079298	8000.552950	10.226931	-0.049520	4.815809
237.904456	8000.533042	10.231936	-0.049488	4.815804
238.011241	8000.469659	10.236941	-0.049508	4.815785
237.941194	8000.561403	10.241946	-0.049495	4.815812
238.010813	8000.570009	10.246951	-0.049508	4.815814
238.045467	8000.568441	10.251955	-0.049514	4.815814
238.167106	8000.550134	10.256960	-0.049537	4.815808
238.208653	8000.547610	10.261965	-0.049545	4.815807
238.022131	8000.533918	10.266970	-0.049510	4.815804
238.029039	8000.480660	10.271975	-0.049512	4.815788
238.197709	8000.558124	10.276979	-0.049543	4.815810
238.230548	8000.558661	10.281984	-0.049549	4.815810
238.279988	8000.569075	10.286989	-0.049559	4.815813
238.185951	8000.516316	10.291994	-0.049541	4.815798
238.303770	8000.564133	10.296999	-0.049563	4.815811
238.116207	8000.548289	10.302003	-0.049528	4.815808
238.082536	8000.561627	10.307008	-0.049522	4.815812
238.314808	8000.566463	10.312013	-0.049565	4.815812
238.109783	8000.554606	10.317018	-0.049527	4.815809
238.388296	8000.574070	10.322023	-0.049579	4.815814
238.185247	8000.454426	10.327027	-0.049541	4.815780
238.168896	8000.564120	10.332032	-0.049538	4.815812
238.255243	8000.501473	10.337037	-0.049555	4.815793
238.078751	8000.556265	10.342042	-0.049522	4.815810
238.265388	8000.545417	10.347047	-0.049557	4.815806
238.394141	8000.552846	10.352051	-0.049581	4.815808
238.263332	8000.557137	10.357056	-0.049556	4.815809
238.230002	8000.555534	10.362061	-0.049550	4.815809
238.108777	8000.531158	10.367066	-0.049528	4.815803
238.425047	8000.549098	10.372071	-0.049587	4.815806
238.376560	8000.551520	10.377075	-0.049578	4.815807
238.107480	8000.539692	10.382080	-0.049528	4.815805
238.144877	8000.562722	10.387085	-0.049535	4.815812
237.959601	8000.529835	10.392090	-0.049500	4.815803
238.002982	8000.460087	10.397095	-0.049508	4.815782
238.037008	8000.555652	10.402099	-0.049515	4.815810
237.788002	8000.519598	10.407104	-0.049468	4.815801
238.297171	8000.544933	10.412109	-0.049563	4.815806
238.170845	8000.533284	10.417114	-0.049540	4.815803
238.153154	8000.569298	10.422119	-0.049537	4.815813
238.102938	8000.564219	10.427123	-0.049527	4.815812
237.958398	8000.546938	10.432128	-0.049500	4.815808
238.501237	8000.473539	10.437133	-0.049602	4.815784
238.205946	8000.532811	10.442138	-0.049547	4.815803
238.202596	8000.565855	10.447143	-0.049546	4.815812
238.466869	8000.574413	10.452147	-0.049595	4.815813
238.374176	8000.564376	10.457152	-0.049578	4.815811
238.313825	8000.490812	10.462157	-0.049567	4.815790
238.311744	8000.565510	10.467162	-0.049567	4.815812
238.008724	8000.579821	10.472167	-0.049510	4.815817
237.950013	8000.569267	10.477171	-0.049499	4.815814
238.205962	8000.470938	10.482176	-0.049547	4.815784
238.176225	8000.557998	10.487181	-0.049542	4.815810
238.001805	8000.522084	10.492186	-0.049509	4.815800
238.298492	8000.551449	10.497191	-0.049565	4.815808
238.272474	8000.556370	10.502195	-0.049560	4.815809
238.365068	8000.565349	10.507200	-0.049577	4.815811
238.343200	8000.559662	10.512205	-0.049573	4.815810
238.237162	8000.470413	10.517210	-0.049553	4.815784
238.434652	8000.584640	10.522215	-0.049590	4.815817
238.284985	8000.557667	10.527219	-0.049562	4.815809
238.331510	8000.555224	10.532224	-0.049571	4.815808
238.231455	8000.477814	10.537229	-0.049552	4.815786
238.211957	8000.543689	10.542234	-0.049549	4.815806
238.015746	8000.536246	10.547239	-0.049512	4.815804
238.138867	8000.558529	10.552243	-0.049535	4.815810
238.160134	8000.511908	10.557248	-0.049539	4.815797
238.194395	8000.547696	10.562253	-0.049546	4.815807
238.293396	8000.545036	10.567258	-0.049564	4.815806
238.213491	8000.549084	10.572263	-0.049550	4.815807
238.162152	8000.550392	10.577267	-0.049540	4.815808
238.192199	8000.525264	10.582272	-0.049546	4.815800
238.395075	8000.575527	10.587277	-0.049584	4.815814
238.175241	8000.520730	10.592282	-0.049543	4.815799
238.304615	8000.545249	10.597287	-0.049567	4.815806
238.275529	8000.551188	10.602291	-0.049562	4.815808
238.428604	8000.540864	10.607296	-0.049590	4.815804
238.456113	8000.469791	10.612301	-0.049595	4.815783
238.358515	8000.551481	10.617306	-0.049577	4.815807
238.290597	8000.551453	10.622311	-0.049565	4.815808
238.222963	8000.545025	10.627315	-0.049552	4.815806
238.335456	8000.542583	10.632320	-0.049573	4.815805
238.376285	8000.580613	10.637325	-0.049581	4.815816
238.209956	8000.530953	10.642330	-0.049550	4.815802
238.354675	8000.557856	10.647335	-0.049577	4.815809
238.243453	8000.549654	10.652339	-0.049556	4.815807
238.221683	8000.523686	10.657344	-0.049552	4.815800
238.477730	8000.562001	10.662349	-0.049600	4.815810
238.459298	8000.525412	10.667354	-0.049597	4.815799
238.418210	8000.547169	10.672359	-0.049589	4.815806
238.525683	8000.548916	10.677363	-0.049609	4.815806
238.287449	8000.549331	10.682368	-0.049565	4.815807
238.253639	8000.557328	10.687373	-0.049558	4.815809
238.502471	8000.546421	10.692378	-0.049605	4.815805
238.376059	8000.551850	10.697383	-0.049581	4.815807
238.333683	8000.544764	10.702387	-0.049574	4.815805
238.297767	8000.511094	10.707392	-0.049567	4.815796
238.286217	8000.551478	10.712397	-0.049565	4.815808
238.136965	8000.525579	10.717402	-0.049537	4.815801
238.225926	8000.554781	10.722407	-0.049554	4.815809
238.252178	8000.543469	10.727411	-0.049559	4.815805
238.102069	8000.530367	10.732416	-0.049531	4.815802
238.244347	8000.483572	10.737421	-0.049557	4.815788
238.275716	8000.544934	10.742426	-0.049563	4.815806
238.389188	8000.561723	10.747431	-0.049584	4.815810
238.431316	8000.573087	10.752435	-0.049592	4.815813
238.422813	8000.551604	10.757440	-0.049591	4.815807
238.367809	8000.469586	10.762445	-0.049581	4.815783
238.349161	8000.547218	10.767450	-0.049577	4.815806
238.473984	8000.569529	10.772455	-0.049601	4.815812
238.611689	8000.571766	10.777459	-0.049626	4.815812
238.459676	8000.549025	10.782464	-0.049598	4.815806
238.482986	8000.569691	10.787469	-0.049602	4.815812
238.439554	8000.430215	10.792474	-0.049594	4.815771
238.386685	8000.531845	10.797479	-0.049585	4.815801
238.365694	8000.545388	10.802483	-0.049581	4.815805
238.234428	8000.552874	10.807488	-0.049556	4.815808
238.330053	8000.541618	10.812493	-0.049574	4.815804
238.411203	8000.541871	10.817498	-0.049589	4.815804
238.427916	8000.568835	10.822503	-0.049593	4.815812
238.504260	8000.564740	10.827507	-0.049607	4.815810
238.349825	8000.530217	10.832512	-0.049578	4.815801
238.597969	8000.581215	10.837517	-0.049624	4.815815
238.500826	8000.540147	10.842522	-0.049606	4.815803
238.314394	8000.575562	10.847527	-0.049572	4.815814
238.383085	8000.475266	10.852531	-0.049585	4.815785
238.635102	8000.564757	10.857536	-0.049632	4.815810
238.600308	8000.591955	10.862541	-0.049625	4.815818
238.462519	8000.472299	10.867546	-0.049600	4.815784
238.272498	8000.574910	10.872551	-0.049564	4.815814
238.386517	8000.562885	10.877555	-0.049586	4.815810
238.227071	8000.567779	10.882560	-0.049556	4.815813
238.207082	8000.482059	10.887565	-0.049552	4.815788
238.416556	8000.570860	10.892570	-0.049591	4.815813
238.402835	8000.557833	10.897575	-0.049589	4.815809
238.411536	8000.576127	10.902579	-0.049591	4.815814
238.459071	8000.554485	10.907584	-0.049599	4.815808
238.512021	8000.490229	10.912589	-0.049609	4.815789
238.363421	8000.547608	10.917594	-0.049582	4.815806
238.473249	8000.565406	10.922599	-0.049602	4.815811
238.631694	8000.570114	10.927603	-0.049632	4.815811
238.505563	8000.547792	10.932608	-0.049608	4.815805
238.506363	8000.555283	10.937613	-0.049609	4.815808
238.583976	8000.540533	10.942618	-0.049623	4.815803
238.474245	8000.533423	10.947623	-0.049603	4.815801
238.565873	8000.563736	10.952627	-0.049620	4.815810
238.756604	8000.520928	10.957632	-0.049655	4.815796
238.599310	8000.569626	10.962637	-0.049626	4.815811
238.368189	8000.468741	10.967642	-0.049583	4.815783
238.392267	8000.517175	10.972647	-0.049588	4.815797
238.660470	8000.555688	10.977651	-0.049638	4.815807
238.510481	8000.560735	10.982656	-0.049610	4.815809
238.448256	8000.581082	10.987661	-0.049598	4.815815
238.544824	8000.562370	10.992666	-0.049616	4.815809
238.533181	8000.554713	10.997671	-0.049614	4.815807
238.562112	8000.466583	11.002675	-0.049620	4.815781
238.530429	8000.570692	11.007680	-0.049614	4.815812
238.755780	8000.479340	11.012685	-0.049656	4.815784
238.816055	8000.552914	11.017690	-0.049667	4.815805
238.603883	8000.577236	11.022695	-0.049628	4.815813
238.825511	8000.569091	11.027699	-0.049669	4.815810
238.531724	8000.550457	11.032704	-0.049614	4.815806
238.521076	8000.550289	11.037709	-0.049613	4.815806
238.592207	8000.538637	11.042714	-0.049626	4.815802
238.585092	8000.554540	11.047719	-0.049625	4.815807
238.631044	8000.483766	11.052723	-0.049633	4.815786
238.573467	8000.568240	11.057728	-0.049623	4.815811
238.650684	8000.576970	11.062733	-0.049637	4.815813
238.480654	8000.462129	11.067738	-0.049605	4.815780
238.620481	8000.576491	11.072743	-0.049631	4.815813
238.857382	8000.561120	11.077747	-0.049676	4.815808
238.542016	8000.554947	11.082752	-0.049617	4.815807
238.581225	8000.576938	11.087757	-0.049624	4.815813
238.691991	8000.468783	11.092762	-0.049645	4.815781
238.639104	8000.560806	11.097767	-0.049635	4.815808
238.627505	8000.570231	11.102771	-0.049633	4.815811
238.605551	8000.544260	11.107776	-0.049629	4.815804
238.804373	8000.487706	11.112781	-0.049666	4.815786
238.780272	8000.558845	11.117786	-0.049662	4.815807
238.864341	8000.578361	11.122791	-0.049678	4.815813
238.735871	8000.595500	11.127795	-0.049654	4.815818
238.818086	8000.478341	11.132800	-0.049669	4.815784
238.683715	8000.594665	11.137805	-0.049644	4.815818
238.715712	8000.566365	11.142810	-0.049650	4.815810
238.653546	8000.539742	11.147815	-0.049639	4.815802
238.616443	8000.538079	11.152819	-0.049632	4.815802
238.768242	8000.525599	11.157824	-0.049660	4.815798
239.169966	8000.559871	11.162829	-0.049735	4.815806
238.803588	8000.547533	11.167834	-0.049667	4.815804
238.682273	8000.556247	11.172839	-0.049644	4.815807
238.831250	8000.466859	11.177843	-0.049672	4.815780
238.713659	8000.564239	11.182848	-0.049650	4.815809
238.730275	8000.589067	11.187853	-0.049653	4.815816
238.612325	8000.557270	11.192858	-0.049631	4.815808
238.742298	8000.567922	11.197863	-0.049656	4.815810
238.761462	8000.568238	11.202867	-0.049659	4.815810
238.607015	8000.447244	11.207872	-0.049631	4.815775
238.609489	8000.575393	11.212877	-0.049631	4.815813
238.754784	8000.549997	11.217882	-0.049658	4.815805
238.666896	8000.559253	11.222887	-0.049642	4.815808
239.028322	8000.505335	11.227891	-0.049709	4.815790
238.701074	8000.570493	11.232896	-0.049648	4.815811
238.640825	8000.572725	11.237901	-0.049637	4.815812
238.778278	8000.474610	11.242906	-0.049663	4.815783
238.854968	8000.581544	11.247911	-0.049677	4.815813
238.987538	8000.583698	11.252915	-0.049702	4.815813
238.847567	8000.555814	11.257920	-0.049676	4.815806
238.823140	8000.488168	11.262925	-0.049671	4.815786
238.756356	8000.463606	11.267930	-0.049659	4.815779
238.728984	8000.578461	11.272935	-0.049654	4.815813
238.814725	8000.576653	11.277939	-0.049670	4.815812
238.690218	8000.546885	11.282944	-0.049647	4.815804
238.637798	8000.572729	11.287949	-0.049637	4.815812
238.748060	8000.563846	11.292954	-0.049658	4.815809
238.873609	8000.550940	11.297959	-0.049681	4.815804
238.942925	8000.444248	11.302963	-0.049694	4.815773
238.707351	8000.552526	11.307968	-0.049651	4.815806
238.951584	8000.538342	11.312973	-0.049696	4.815800
238.682489	8000.553201	11.317978	-0.049646	4.815806
238.632269	8000.534245	11.322983	-0.049637	4.815801
238.941859	8000.581969	11.327987	-0.049694	4.815813
238.890565	8000.518158	11.332992	-0.049685	4.815795
238.971273	8000.577119	11.337997	-0.049700	4.815812
239.092870	8000.443518	11.343002	-0.049723	4.815772
239.032464	8000.542893	11.348007	-0.049712	4.815801
239.037680	8000.561131	11.353011	-0.049713	4.815807
238.929340	8000.552975	11.358016	-0.049692	4.815805
238.966210	8000.584536	11.363021	-0.049699	4.815814
238.868974	8000.547737	11.368026	-0.049681	4.815803
238.741335	8000.537133	11.373031	-0.049658	4.815801
238.745398	8000.570298	11.378035	-0.049658	4.815811
238.736689	8000.562689	11.383040	-0.049657	4.815808
238.916005	8000.480198	11.388045	-0.049690	4.815784
238.761354	8000.567369	11.393050	-0.049662	4.815810
238.637150	8000.481027	11.398055	-0.049638	4.815785
238.906824	8000.578278	11.403059	-0.049689	4.815812
238.807425	8000.560659	11.408064	-0.049670	4.815808
238.842041	8000.569766	11.413069	-0.049677	4.815810
239.015015	8000.570440	11.418074	-0.049709	4.815809
238.982664	8000.483450	11.423079	-0.049703	4.815784
238.850591	8000.579528	11.428083	-0.049679	4.815813
238.877449	8000.552213	11.433088	-0.049684	4.815805
238.909697	8000.571956	11.438093	-0.049690	4.815810
238.837837	8000.455503	11.443098	-0.049676	4.815777
238.785328	8000.574221	11.448103	-0.049667	4.815812
238.937901	8000.572429	11.453107	-0.049695	4.815810
238.759781	8000.538589	11.458112	-0.049662	4.815801
238.745971	8000.573599	11.463117	-0.049660	4.815812
238.925785	8000.491116	11.468122	-0.049693	4.815787
238.860446	8000.547709	11.473127	-0.049681	4.815803
238.807434	8000.577814	11.478131	-0.049671	4.815813
238.819222	8000.559862	11.483136	-0.049673	4.815807
238.938558	8000.480669	11.488141	-0.049696	4.815784
238.902092	8000.566554	11.493146	-0.049689	4.815809
238.935287	8000.555354	11.498151	-0.049695	4.815805
238.899490	8000.592143	11.503155	-0.049689	4.815816
238.903444	8000.447028	11.508160	-0.049689	4.815774
238.919402	8000.577531	11.513165	-0.049692	4.815812
238.912500	8000.562479	11.518170	-0.049691	4.815808
238.982452	8000.550807	11.523175	-0.049704	4.815804
239.061402	8000.573443	11.528179	-0.049719	4.815810
239.089008	8000.482087	11.533184	-0.049724	4.815783
239.040664	8000.578455	11.538189	-0.049715	4.815812
239.031191	8000.556956	11.543194	-0.049714	4.815805
238.739398	8000.544759	11.548199	-0.049659	4.815803
238.887354	8000.574919	11.553203	-0.049687	4.815811
238.764632	8000.551584	11.558208	-0.049664	4.815805
238.792486	8000.584067	11.563213	-0.049669	4.815814
238.732049	8000.564944	11.568218	-0.049658	4.815809
238.760337	8000.466128	11.573223	-0.049664	4.815780
239.135143	8000.578962	11.578227	-0.049733	4.815811
239.047188	8000.532704	11.583232	-0.049717	4.815798
238.992189	8000.591600	11.588237	-0.049707	4.815816
239.007049	8000.481890	11.593242	-0.049710	4.815784
238.829254	8000.564417	11.598247	-0.049677	4.815808
239.054715	8000.591562	11.603251	-0.049719	4.815815
239.014933	8000.577045	11.608256	-0.049711	4.815811
239.032382	8000.475917	11.613261	-0.049715	4.815782
238.993337	8000.535071	11.618266	-0.049708	4.815799
238.826410	8000.544114	11.623271	-0.049676	4.815803
239.000705	8000.578970	11.628275	-0.049709	4.815812
238.849455	8000.562646	11.633280	-0.049681	4.815808
239.019038	8000.573940	11.638285	-0.049713	4.815810
238.992795	8000.478509	11.643290	-0.049708	4.815783
238.822504	8000.565428	11.648295	-0.049676	4.815809
239.041030	8000.590326	11.653299	-0.049717	4.815815
239.033207	8000.456762	11.658304	-0.049715	4.815776
238.964062	8000.582683	11.663309	-0.049703	4.815813
239.136103	8000.572667	11.668314	-0.049735	4.815809
238.998891	8000.557638	11.673319	-0.049709	4.815806
239.074737	8000.478807	11.678323	-0.049723	4.815782
238.878871	8000.545027	11.683328	-0.049687	4.815803
239.013013	8000.577098	11.688333	-0.049712	4.815811
239.001542	8000.572647	11.693338	-0.049710	4.815810
239.031518	8000.575274	11.698343	-0.049716	4.815811
239.048818	8000.569154	11.703347	-0.049719	4.815809
239.074734	8000.549296	11.708352	-0.049724	4.815803
238.980338	8000.486922	11.713357	-0.049706	4.815785
239.049766	8000.512606	11.718362	-0.049719	4.815792
238.968182	8000.555058	11.723367	-0.049704	4.815805
239.238869	8000.602153	11.728371	-0.049755	4.815818
239.108479	8000.554140	11.733376	-0.049730	4.815804
239.080885	8000.470430	11.738381	-0.049725	4.815780
239.155090	8000.568784	11.743386	-0.049739	4.815808
238.987800	8000.546862	11.748391	-0.049708	4.815803
238.980135	8000.585174	11.753395	-0.049707	4.815814
239.194865	8000.541688	11.758400	-0.049747	4.815800
239.093708	8000.555000	11.763405	-0.049728	4.815804
239.079021	8000.473634	11.768410	-0.049725	4.815781
239.129645	8000.557728	11.773415	-0.049735	4.815805
239.230854	8000.575387	11.778419	-0.049754	4.815810
239.095209	8000.546505	11.783424	-0.049728	4.815802
239.202058	8000.584539	11.788429	-0.049748	4.815813
239.308548	8000.568122	11.793434	-0.049768	4.815807
239.165894	8000.573288	11.798439	-0.049742	4.815809
239.188418	8000.496795	11.803443	-0.049746	4.815787
239.188298	8000.565121	11.808448	-0.049746	4.815807
239.056288	8000.583270	11.813453	-0.049722	4.815813
239.044622	8000.529709	11.818458	-0.049719	4.815797
238.981648	8000.494532	11.823463	-0.049708	4.815787
238.954526	8000.567758	11.828467	-0.049703	4.815809
238.937524	8000.549339	11.833472	-0.049700	4.815803
238.919279	8000.593886	11.838477	-0.049696	4.815817
239.037646	8000.484785	11.843482	-0.049718	4.815784
239.020787	8000.575258	11.848487	-0.049715	4.815811
238.973792	8000.502977	11.853491	-0.049707	4.815790
239.042940	8000.571358	11.858496	-0.049720	4.815809
239.139250	8000.573992	11.863501	-0.049738	4.815810
239.123449	8000.481932	11.868506	-0.049735	4.815783
239.017961	8000.572036	11.873511	-0.049715	4.815810
239.026295	8000.582852	11.878515	-0.049717	4.815813
239.005861	8000.579324	11.883520	-0.049713	4.815812
239.098365	8000.554140	11.888525	-0.049730	4.815804
239.262809	8000.476745	11.893530	-0.049761	4.815781
239.290046	8000.573271	11.898535	-0.049766	4.815809
239.222607	8000.578588	11.903539	-0.049754	4.815811
239.208838	8000.474818	11.908544	-0.049751	4.815780
239.083411	8000.588085	11.913549	-0.049728	4.815814
239.368933	8000.483829	11.918554	-0.049781	4.815782
239.096590	8000.543473	11.923559	-0.049730	4.815801
239.041205	8000.570336	11.928563	-0.049720	4.815809
239.072061	8000.561234	11.933568	-0.049726	4.815806
239.034868	8000.585190	11.938573	-0.049719	4.815813
239.056913	8000.473461	11.943578	-0.049723	4.815781
239.030731	8000.570188	11.948583	-0.049719	4.815809
239.280780	8000.578517	11.953587	-0.049765	4.815810
239.052818	8000.555611	11.958592	-0.049723	4.815805
239.157859	8000.578670	11.963597	-0.049742	4.815811
239.214170	8000.460023	11.968602	-0.049753	4.815776
239.339604	8000.569883	11.973607	-0.049776	4.815808
239.179806	8000.592919	11.978611	-0.049747	4.815815
239.028919	8000.465576	11.983616	-0.049719	4.815779
239.197536	8000.580407	11.988621	-0.049750	4.815811
239.337026	8000.559187	11.993626	-0.049776	4.815804
239.267844	8000.576219	11.998631	-0.049763	4.815810
239.125440	8000.487445	12.003635	-0.049737	4.815784
239.273070	8000.565639	12.008640	-0.049764	4.815807
239.364856	8000.603429	12.013645	-0.049782	4.815817
239.403690	8000.493039	12.018650	-0.049789	4.815785
239.277552	8000.599889	12.023655	-0.049765	4.815817
239.218866	8000.484716	12.028659	-0.049754	4.815783
238.985534	8000.476669	12.033664	-0.049711	4.815782
239.153377	8000.595757	12.038669	-0.049742	4.815816
239.129993	8000.574032	12.043674	-0.049738	4.815810
239.058202	8000.565401	12.048679	-0.049725	4.815808
239.314208	8000.495896	12.053683	-0.049773	4.815786
239.222047	8000.580878	12.058688	-0.049755	4.815811
239.229262	8000.589541	12.063693	-0.049757	4.815814
239.098684	8000.482810	12.068698	-0.049733	4.815783
239.247901	8000.586651	12.073703	-0.049760	4.815813
239.395467	8000.511117	12.078707	-0.049788	4.815790
239.245351	8000.492676	12.083712	-0.049760	4.815785
239.289922	8000.494471	12.088717	-0.049768	4.815786
239.233834	8000.482892	12.093722	-0.049758	4.815783
238.973149	8000.580088	12.098727	-0.049710	4.815812
239.176570	8000.504393	12.103731	-0.049748	4.815789
239.018525	8000.588307	12.108736	-0.049718	4.815814
239.074813	8000.483538	12.113741	-0.049729	4.815784
239.015409	8000.588267	12.118746	-0.049718	4.815814
238.976948	8000.518259	12.123751	-0.049711	4.815794
239.110933	8000.557800	12.128755	-0.049736	4.815805
239.081071	8000.545578	12.133760	-0.049730	4.815802
239.136818	8000.580649	12.138765	-0.049741	4.815812
239.231231	8000.578982	12.143770	-0.049758	4.815811
239.201009	8000.482418	12.148775	-0.049753	4.815783
239.199408	8000.584882	12.153779	-0.049752	4.815813
239.323071	8000.571946	12.158784	-0.049775	4.815808
239.321446	8000.576195	12.163789	-0.049775	4.815809
239.218578	8000.569195	12.168794	-0.049756	4.815808
239.103254	8000.438159	12.173799	-0.049735	4.815770
239.223404	8000.583162	12.178803	-0.049757	4.815812
239.115678	8000.564340	12.183808	-0.049737	4.815807
238.970375	8000.578003	12.188813	-0.049710	4.815812
239.153378	8000.579908	12.193818	-0.049744	4.815811
239.238723	8000.556743	12.198823	-0.049760	4.815804
239.171183	8000.508681	12.203827	-0.049748	4.815790
239.380356	8000.563320	12.208832	-0.049787	4.815805
239.251348	8000.577247	12.213837	-0.049763	4.815810
239.100086	8000.504342	12.218842	-0.049735	4.815789
239.195143	8000.535780	12.223847	-0.049752	4.815798
239.323982	8000.585913	12.228851	-0.049777	4.815812
239.153690	8000.553266	12.233856	-0.049745	4.815803
239.112310	8000.546196	12.238861	-0.049737	4.815802
239.371564	8000.469270	12.243866	-0.049785	4.815778
239.232803	8000.530011	12.248871	-0.049760	4.815796
239.418740	8000.569328	12.253875	-0.049794	4.815807
239.447866	8000.552724	12.258880	-0.049800	4.815802
239.394551	8000.557203	12.263885	-0.049790	4.815803
239.260662	8000.565713	12.268890	-0.049765	4.815807
239.236759	8000.535440	12.273895	-0.049761	4.815798
239.484977	8000.497834	12.278899	-0.049807	4.815786
239.332414	8000.564757	12.283904	-0.049779	4.815806
239.309019	8000.576126	12.288909	-0.049774	4.815809
239.292623	8000.571595	12.293914	-0.049771	4.815808
239.391414	8000.546514	12.298919	-0.049790	4.815800
239.359543	8000.569488	12.303923	-0.049784	4.815807
239.268864	8000.553078	12.308928	-0.049767	4.815803
239.334800	8000.483694	12.313933	-0.049780	4.815782
239.293574	8000.559894	12.318938	-0.049772	4.815805
239.160560	8000.542798	12.323943	-0.049747	4.815800
239.364588	8000.585610	12.328947	-0.049785	4.815812
239.369756	8000.572888	12.333952	-0.049786	4.815808
239.280944	8000.487117	12.338957	-0.049770	4.815784
239.618816	8000.583342	12.343962	-0.049833	4.815810
239.389510	8000.555076	12.348967	-0.049790	4.815803
239.364027	8000.579222	12.353971	-0.049785	4.815810
239.251066	8000.551775	12.358976	-0.049765	4.815803
239.574577	8000.536741	12.363981	-0.049825	4.815797
239.433641	8000.560083	12.368986	-0.049799	4.815804
239.314744	8000.529337	12.373991	-0.049777	4.815796
239.320242	8000.572133	12.378995	-0.049778	4.815808
239.217557	8000.565136	12.384000	-0.049759	4.815807
239.281577	8000.571517	12.389005	-0.049771	4.815808
239.357891	8000.486288	12.394010	-0.049785	4.815783
239.284499	8000.545954	12.399015	-0.049771	4.815801
239.400490	8000.569190	12.404019	-0.049793	4.815807
239.412039	8000.559775	12.409024	-0.049795	4.815804
239.457740	8000.560521	12.414029	-0.049804	4.815804
239.698459	8000.562294	12.419034	-0.049849	4.815803
239.490541	8000.561063	12.424039	-0.049810	4.815804
239.622999	8000.595243	12.429043	-0.049835	4.815813
239.611580	8000.568374	12.434048	-0.049833	4.815806
239.302423	8000.577245	12.439053	-0.049775	4.815810
239.124022	8000.571156	12.444058	-0.049742	4.815809
239.309648	8000.549617	12.449063	-0.049777	4.815802
239.347513	8000.476575	12.454067	-0.049784	4.815780
239.322506	8000.537025	12.459072	-0.049779	4.815798
239.298980	8000.540919	12.464077	-0.049775	4.815799
239.470842	8000.574670	12.469082	-0.049807	4.815808
239.363981	8000.533443	12.474087	-0.049787	4.815797
239.359407	8000.586752	12.479091	-0.049786	4.815812
239.311571	8000.552888	12.484096	-0.049777	4.815803
239.180044	8000.590260	12.489101	-0.049753	4.815814
239.138520	8000.481770	12.494106	-0.049745	4.815783
239.308833	8000.553927	12.499111	-0.049777	4.815803
239.370597	8000.591230	12.504115	-0.049789	4.815813
239.324266	8000.561660	12.509120	-0.049780	4.815805
239.439568	8000.572075	12.514125	-0.049801	4.815808
239.496782	8000.569806	12.519130	-0.049812	4.815807
239.352107	8000.531169	12.524135	-0.049785	4.815796
239.442496	8000.518761	12.529139	-0.049802	4.815792
239.316197	8000.484693	12.534144	-0.049779	4.815783
239.335623	8000.574687	12.539149	-0.049782	4.815809
239.387118	8000.559514	12.544154	-0.049792	4.815804
239.144325	8000.567326	12.549159	-0.049747	4.815808
239.326269	8000.497688	12.554163	-0.049781	4.815786
239.334247	8000.542659	12.559168	-0.049782	4.815799
239.344059	8000.572715	12.564173	-0.049784	4.815808
239.445601	8000.577569	12.569178	-0.049803	4.815809
239.304358	8000.546461	12.574183	-0.049777	4.815801
239.437988	8000.582794	12.579187	-0.049802	4.815811
239.402771	8000.558742	12.584192	-0.049795	4.815804
239.301475	8000.574186	12.589197	-0.049777	4.815809
239.222258	8000.486436	12.594202	-0.049762	4.815784
239.308124	8000.561494	12.599207	-0.049778	4.815805
239.458919	8000.588498	12.604211	-0.049806	4.815812
239.270829	8000.469091	12.609216	-0.049771	4.815778
239.160996	8000.573003	12.614221	-0.049751	4.815809
239.283732	8000.585673	12.619226	-0.049774	4.815812
239.212292	8000.566372	12.624231	-0.049761	4.815807
239.101976	8000.494131	12.629235	-0.049740	4.815786
239.231523	8000.566694	12.634240	-0.049764	4.815807
239.407086	8000.553533	12.639245	-0.049797	4.815802
239.484752	8000.591094	12.644250	-0.049812	4.815813
239.377258	8000.573343	12.649255	-0.049792	4.815808
239.538726	8000.500170	12.654259	-0.049822	4.815786
239.479005	8000.576071	12.659264	-0.049811	4.815808
239.482162	8000.486453	12.664269	-0.049811	4.815782
239.472552	8000.586652	12.669274	-0.049810	4.815812
239.559693	8000.581665	12.674279	-0.049826	4.815810
239.407076	8000.491657	12.679283	-0.049797	4.815784
239.528914	8000.581177	12.684288	-0.049820	4.815810
239.368390	8000.557228	12.689293	-0.049790	4.815803
239.267962	8000.594037	12.694298	-0.049772	4.815815
239.324079	8000.538372	12.699303	-0.049782	4.815798
239.454167	8000.471096	12.704307	-0.049806	4.815778
239.407930	8000.564296	12.709312	-0.049798	4.815805
239.214252	8000.566499	12.714317	-0.049762	4.815807
239.485669	8000.577310	12.719322	-0.049813	4.815809
239.342005	8000.549365	12.724327	-0.049786	4.815801
239.271587	8000.582390	12.729331	-0.049773	4.815811
239.451802	8000.587452	12.734336	-0.049806	4.815812
239.512028	8000.525448	12.739341	-0.049818	4.815793
239.642136	8000.564928	12.744346	-0.049842	4.815804
239.633445	8000.447361	12.749351	-0.049840	4.815770
239.670592	8000.579278	12.754355	-0.049847	4.815808
239.446496	8000.559636	12.759360	-0.049806	4.815804
239.542593	8000.563335	12.764365	-0.049824	4.815804
239.728863	8000.582374	12.769370	-0.049858	4.815809
239.346785	8000.564441	12.774375	-0.049787	4.815806
239.358685	8000.514464	12.779379	-0.049790	4.815791
239.470478	8000.562187	12.784384	-0.049811	4.815804
239.439740	8000.560626	12.789389	-0.049805	4.815804
239.604663	8000.481104	12.794394	-0.049836	4.815780
239.604356	8000.543022	12.799399	-0.049836	4.815798
239.616829	8000.591270	12.804403	-0.049838	4.815812
239.749575	8000.565671	12.809408	-0.049863	4.815804
239.557840	8000.566837	12.814413	-0.049827	4.815805
239.722951	8000.583398	12.819418	-0.049858	4.815809
239.626871	8000.567967	12.824423	-0.049840	4.815805
239.529965	8000.579212	12.829427	-0.049822	4.815809
239.629623	8000.463402	12.834432	-0.049841	4.815775
239.572181	8000.561759	12.839437	-0.049830	4.815804
239.608018	8000.566615	12.844442	-0.049837	4.815805
239.576570	8000.543692	12.849447	-0.049831	4.815798
239.510631	8000.561844	12.854451	-0.049819	4.815804
239.525294	8000.553547	12.859456	-0.049822	4.815802
239.459505	8000.566364	12.864461	-0.049809	4.815806
239.564322	8000.586217	12.869466	-0.049829	4.815811
239.592947	8000.563200	12.874471	-0.049834	4.815804
239.688834	8000.574368	12.879475	-0.049852	4.815807
239.374411	8000.560735	12.884480	-0.049794	4.815804
239.509987	8000.565073	12.889485	-0.049819	4.815805
239.661654	8000.492809	12.894490	-0.049847	4.815783
239.533682	8000.562266	12.899495	-0.049824	4.815804
239.610992	8000.581673	12.904499	-0.049838	4.815809
239.516687	8000.575879	12.909504	-0.049821	4.815808
239.428837	8000.574460	12.914509	-0.049804	4.815808
239.648159	8000.491549	12.919514	-0.049845	4.815783
239.640150	8000.560816	12.924519	-0.049844	4.815803
239.842809	8000.583323	12.929523	-0.049882	4.815809
239.793434	8000.577190	12.934528	-0.049872	4.815807
239.746081	8000.570022	12.939533	-0.049864	4.815805
239.673949	8000.509074	12.944538	-0.049850	4.815788
239.491046	8000.576573	12.949543	-0.049816	4.815808
239.594294	8000.498186	12.954547	-0.049836	4.815785
239.704773	8000.561900	12.959552	-0.049856	4.815803
239.544306	8000.544358	12.964557	-0.049826	4.815799
239.445625	8000.575858	12.969562	-0.049808	4.815808
239.570090	8000.573611	12.974567	-0.049831	4.815807
239.676310	8000.589217	12.979571	-0.049851	4.815811
239.711547	8000.488375	12.984576	-0.049858	4.815782
239.587235	8000.582445	12.989581	-0.049835	4.815810
239.705992	8000.579038	12.994586	-0.049857	4.815808
239.427886	8000.556386	12.999591	-0.049805	4.815803
239.525173	8000.571847	13.004595	-0.049823	4.815807
239.559909	8000.479538	13.009600	-0.049830	4.815780
239.492250	8000.592675	13.014605	-0.049817	4.815813
239.661477	8000.585816	13.019610	-0.049849	4.815810
239.720609	8000.521659	13.024615	-0.049860	4.815791
239.464235	8000.562345	13.029619	-0.049812	4.815804
239.484387	8000.467665	13.034624	-0.049816	4.815777
239.396130	8000.575129	13.039629	-0.049800	4.815808
239.719368	8000.593186	13.044634	-0.049860	4.815812
239.630882	8000.549054	13.049639	-0.049844	4.815800
239.774833	8000.600502	13.054643	-0.049871	4.815814
239.898724	8000.455192	13.059648	-0.049894	4.815771
239.654738	8000.556930	13.064653	-0.049848	4.815802
239.653405	8000.590008	13.069658	-0.049848	4.815812
239.577422	8000.573835	13.074663	-0.049834	4.815807
239.609805	8000.585041	13.079667	-0.049840	4.815810
239.548484	8000.459149	13.084672	-0.049829	4.815774
239.748381	8000.581961	13.089677	-0.049866	4.815809
239.605884	8000.587129	13.094682	-0.049840	4.815811
239.657514	8000.570890	13.099687	-0.049849	4.815806
239.598502	8000.488804	13.104691	-0.049838	4.815782
239.604363	8000.555093	13.109696	-0.049839	4.815802
239.484298	8000.573435	13.114701	-0.049817	4.815808
239.680148	8000.505090	13.119706	-0.049854	4.815787
239.462553	8000.551742	13.124711	-0.049813	4.815801
239.549837	8000.573446	13.129715	-0.049830	4.815807
239.514317	8000.583551	13.134720	-0.049823	4.815810
239.440860	8000.549271	13.139725	-0.049809	4.815801
239.714924	8000.582544	13.144730	-0.049860	4.815809
239.516167	8000.456558	13.149735	-0.049823	4.815773
239.692281	8000.600336	13.154739	-0.049856	4.815814
239.810110	8000.577698	13.159744	-0.049878	4.815807
239.665992	8000.462206	13.164749	-0.049851	4.815774
239.567773	8000.586590	13.169754	-0.049833	4.815811
239.642047	8000.545097	13.174759	-0.049847	4.815798
239.679433	8000.578803	13.179763	-0.049854	4.815808
239.422599	8000.556496	13.184768	-0.049806	4.815803
239.438709	8000.531141	13.189773	-0.049810	4.815795
239.599838	8000.562583	13.194778	-0.049840	4.815804
239.584542	8000.535651	13.199783	-0.049837	4.815796
239.618642	8000.565033	13.204787	-0.049843	4.815804
239.645688	8000.566545	13.209792	-0.049848	4.815805
239.487776	8000.537301	13.214797	-0.049819	4.815797
239.593147	8000.578514	13.219802	-0.049839	4.815808
239.874777	8000.553194	13.224807	-0.049891	4.815800
239.827547	8000.533218	13.229811	-0.049882	4.815794
239.574556	8000.460797	13.234816	-0.049835	4.815774
239.618427	8000.527702	13.239821	-0.049844	4.815793
239.708896	8000.575080	13.244826	-0.049861	4.815807
239.618961	8000.533059	13.249831	-0.049844	4.815795
239.632347	8000.582389	13.254835	-0.049846	4.815809
239.824613	8000.565229	13.259840	-0.049882	4.815803
239.559822	8000.540657	13.264845	-0.049833	4.815798
239.547786	8000.585304	13.269850	-0.049831	4.815811
239.758299	8000.586588	13.274855	-0.049870	4.815810
239.810400	8000.585303	13.279859	-0.049880	4.815809
239.674202	8000.482749	13.284864	-0.049854	4.815780
239.666979	8000.566975	13.289869	-0.049853	4.815805
239.879382	8000.582167	13.294874	-0.049893	4.815808
239.519444	8000.563525	13.299879	-0.049826	4.815804
239.775907	8000.595446	13.304883	-0.049874	4.815813
239.911725	8000.403357	13.309888	-0.049899	4.815756
239.605012	8000.589483	13.314893	-0.049842	4.815812
239.751676	8000.509664	13.319898	-0.049869	4.815788
239.639883	8000.582586	13.324903	-0.049849	4.815809
239.721200	8000.482491	13.329907	-0.049864	4.815780
239.822919	8000.594105	13.334912	-0.049883	4.815812
239.655868	8000.496388	13.339917	-0.049852	4.815784
239.658176	8000.499634	13.344922	-0.049852	4.815785
239.681079	8000.561929	13.349927	-0.049857	4.815803
239.667221	8000.580926	13.354931	-0.049854	4.815809
239.592196	8000.560498	13.359936	-0.049840	4.815803
239.621666	8000.557779	13.364941	-0.049846	4.815802
239.731378	8000.593725	13.369946	-0.049866	4.815812
239.601519	8000.446437	13.374951	-0.049842	4.815770
239.869962	8000.573564	13.379955	-0.049892	4.815806
239.713323	8000.562489	13.384960	-0.049863	4.815803
239.368388	8000.568644	13.389965	-0.049799	4.815807
239.794251	8000.577690	13.394970	-0.049878	4.815807
239.902181	8000.523932	13.399975	-0.049898	4.815791
239.598739	8000.591611	13.404979	-0.049842	4.815812
239.706616	8000.470596	13.409984	-0.049862	4.815776
239.793417	8000.562752	13.414989	-0.049878	4.815803
239.772673	8000.588042	13.419994	-0.049875	4.815810
239.558868	8000.562162	13.424999	-0.049835	4.815804
239.897185	8000.598612	13.430003	-0.049898	4.815813
239.709004	8000.489878	13.435008	-0.049863	4.815782
239.590452	8000.570163	13.440013	-0.049841	4.815806
239.733363	8000.597039	13.445018	-0.049868	4.815813
239.547615	8000.579087	13.450023	-0.049833	4.815809
239.657166	8000.541369	13.455027	-0.049853	4.815797
239.548381	8000.480895	13.460032	-0.049833	4.815780
239.786940	8000.568037	13.465037	-0.049878	4.815804
239.701193	8000.586936	13.470042	-0.049862	4.815810
239.592494	8000.561692	13.475047	-0.049842	4.815803
239.682248	8000.573829	13.480051	-0.049858	4.815807
239.780096	8000.578623	13.485056	-0.049877	4.815808
239.551352	8000.547163	13.490061	-0.049834	4.815799
239.631690	8000.584768	13.495066	-0.049849	4.815810
239.735361	8000.475428	13.500071	-0.049868	4.815778
239.663686	8000.605581	13.505075	-0.049855	4.815816
239.773746	8000.572141	13.510080	-0.049876	4.815806
239.450004	8000.548749	13.515085	-0.049816	4.815800
239.627917	8000.470504	13.520090	-0.049849	4.815777
239.594419	8000.569249	13.525095	-0.049843	4.815806
239.754526	8000.548364	13.530099	-0.049872	4.815799
239.717793	8000.575531	13.535104	-0.049866	4.815807
239.640834	8000.576423	13.540109	-0.049851	4.815808
239.718057	8000.508289	13.545114	-0.049866	4.815787
239.565879	8000.562408	13.550119	-0.049838	4.815804
239.577323	8000.567936	13.555123	-0.049840	4.815805
239.800317	8000.581166	13.560128	-0.049881	4.815808
239.753825	8000.575079	13.565133	-0.049873	4.815807
239.782004	8000.492272	13.570138	-0.049878	4.815782
239.546711	8000.542907	13.575143	-0.049834	4.815798
239.451478	8000.585138	13.580147	-0.049817	4.815811
239.847925	8000.577694	13.585152	-0.049891	4.815807
239.497612	8000.556005	13.590157	-0.049825	4.815802
239.507046	8000.574312	13.595162	-0.049827	4.815808
239.577246	8000.566915	13.600167	-0.049840	4.815805
239.393115	8000.558597	13.605171	-0.049806	4.815803
239.669408	8000.508637	13.610176	-0.049858	4.815788
239.591948	8000.562899	13.615181	-0.049843	4.815804
239.725420	8000.569339	13.620186	-0.049868	4.815805
239.579697	8000.538157	13.625191	-0.049841	4.815797
239.735381	8000.583389	13.630195	-0.049870	4.815809
239.757931	8000.491950	13.635200	-0.049874	4.815782
239.624672	8000.567726	13.640205	-0.049850	4.815805
239.606670	8000.505521	13.645210	-0.049846	4.815787
239.394565	8000.570411	13.650215	-0.049807	4.815807
239.493521	8000.573089	13.655219	-0.049825	4.815807
239.677698	8000.493878	13.660224	-0.049860	4.815783
239.564812	8000.572120	13.665229	-0.049839	4.815807
239.482310	8000.487518	13.670234	-0.049823	4.815782
239.545066	8000.578216	13.675239	-0.049835	4.815808
239.597695	8000.575872	13.680243	-0.049845	4.815808
239.816329	8000.584760	13.685248	-0.049886	4.815809
239.567840	8000.543372	13.690253	-0.049840	4.815798
239.510880	8000.586223	13.695258	-0.049829	4.815811
239.600353	8000.551382	13.700263	-0.049846	4.815800
239.767734	8000.472967	13.705267	-0.049877	4.815777
239.557527	8000.564577	13.710272	-0.049838	4.815804
239.474924	8000.561108	13.715277	-0.049823	4.815804
239.711994	8000.579903	13.720282	-0.049867	4.815808
239.650883	8000.551160	13.725287	-0.049856	4.815800
239.604304	8000.584572	13.730291	-0.049847	4.815810
239.725861	8000.582278	13.735296	-0.049870	4.815809
239.579112	8000.477419	13.740301	-0.049842	4.815779
239.658294	8000.605747	13.745306	-0.049857	4.815816
239.751793	8000.498378	13.750311	-0.049875	4.815784
239.465039	8000.596219	13.755315	-0.049821	4.815814
239.638288	8000.488007	13.760320	-0.049854	4.815782
239.447571	8000.550041	13.765325	-0.049818	4.815801
239.740803	8000.593233	13.770330	-0.049873	4.815812
239.698895	8000.549857	13.775335	-0.049865	4.815799
239.704807	8000.563836	13.780339	-0.049866	4.815803
239.756598	8000.583897	13.785344	-0.049876	4.815809
239.530043	8000.555675	13.790349	-0.049834	4.815802
239.642532	8000.554302	13.795354	-0.049855	4.815801
239.791703	8000.439294	13.800359	-0.049883	4.815767
239.852479	8000.556649	13.805363	-0.049894	4.815801
239.912780	8000.570443	13.810368	-0.049905	4.815804
239.759322	8000.548744	13.815373	-0.049877	4.815799
239.895377	8000.580847	13.820378	-0.049902	4.815808
239.980257	8000.563013	13.825383	-0.049918	4.815802
239.630488	8000.588305	13.830387	-0.049853	4.815811
239.850282	8000.587605	13.835392	-0.049894	4.815810
239.818620	8000.468597	13.840397	-0.049888	4.815775
239.710816	8000.591759	13.845402	-0.049868	4.815812
239.679267	8000.507983	13.850407	-0.049862	4.815787
239.819884	8000.591403	13.855411	-0.049889	4.815811
239.833453	8000.573480	13.860416	-0.049891	4.815806
239.597123	8000.486383	13.865421	-0.049847	4.815781
239.764037	8000.578770	13.870426	-0.049878	4.815808
239.811004	8000.525091	13.875431	-0.049887	4.815792
239.717768	8000.512909	13.880435	-0.049870	4.815789
239.805217	8000.599738	13.885440	-0.049886	4.815813
239.695425	8000.482666	13.890445	-0.049866	4.815780
239.680136	8000.505910	13.895450	-0.049863	4.815787
239.616815	8000.592428	13.900455	-0.049851	4.815812
239.721133	8000.485234	13.905459	-0.049871	4.815780
239.832428	8000.600205	13.910464	-0.049892	4.815813
239.721992	8000.487393	13.915469	-0.049871	4.815781
240.041579	8000.605743	13.920474	-0.049931	4.815814
239.653472	8000.573833	13.925479	-0.049858	4.815807
239.633771	8000.480641	13.930483	-0.049855	4.815779
239.872607	8000.585937	13.935488	-0.049899	4.815809
239.881064	8000.554053	13.940493	-0.049901	4.815800
239.779513	8000.597249	13.945498	-0.049882	4.815813
239.762948	8000.453933	13.950503	-0.049879	4.815771
239.929919	8000.597564	13.955507	-0.049910	4.815812
239.923212	8000.497109	13.960512	-0.049909	4.815783
239.702612	8000.578942	13.965517	-0.049868	4.815808
239.835103	8000.566150	13.970522	-0.049893	4.815803
239.733987	8000.582664	13.975527	-0.049874	4.815809
239.578403	8000.539579	13.980531	-0.049845	4.815797
239.723428	8000.583571	13.985536	-0.049872	4.815809
239.734041	8000.564532	13.990541	-0.049874	4.815803
239.773874	8000.497927	13.995546	-0.049882	4.815784
239.654614	8000.570728	14.000551	-0.049860	4.815806
239.781036	8000.585594	14.005555	-0.049883	4.815809
239.996178	8000.417210	14.010560	-0.049923	4.815759
239.830412	8000.603486	14.015565	-0.049893	4.815814
239.893095	8000.370712	14.020570	-0.049904	4.815746
239.778234	8000.594110	14.025575	-0.049883	4.815812
239.599544	8000.580542	14.030579	-0.049850	4.815809
239.737413	8000.476027	14.035584	-0.049875	4.815778
239.837601	8000.568400	14.040589	-0.049894	4.815804
239.784586	8000.577153	14.045594	-0.049884	4.815807
239.943663	8000.558387	14.050599	-0.049914	4.815801
239.856102	8000.564445	14.055603	-0.049898	4.815803
240.060002	8000.501568	14.060608	-0.049936	4.815784
239.906596	8000.562072	14.065613	-0.049907	4.815802
239.970033	8000.592998	14.070618	-0.049919	4.815811
239.840654	8000.570621	14.075623	-0.049895	4.815805
239.990776	8000.573061	14.080627	-0.049923	4.815805
239.959960	8000.489297	14.085632	-0.049917	4.815780
239.886732	8000.591668	14.090637	-0.049904	4.815811
239.869168	8000.494240	14.095642	-0.049901	4.815782
239.667295	8000.584918	14.100647	-0.049863	4.815810
239.653499	8000.488619	14.105651	-0.049861	4.815782
239.684490	8000.598018	14.110656	-0.049866	4.815813
239.615307	8000.555266	14.115661	-0.049854	4.815801
239.569207	8000.579078	14.120666	-0.049845	4.815808
239.703297	8000.566312	14.125671	-0.049870	4.815804
239.895150	8000.472280	14.130675	-0.049906	4.815776
239.851854	8000.585812	14.135680	-0.049898	4.815809
239.948681	8000.575645	14.140685	-0.049916	4.815806
240.030410	8000.500111	14.145690	-0.049931	4.815783
239.672426	8000.581851	14.150695	-0.049865	4.815809
239.755552	8000.593880	14.155699	-0.049880	4.815812
239.826148	8000.503220	14.160704	-0.049893	4.815785
239.737845	8000.578658	14.165709	-0.049877	4.815808
239.914348	8000.596471	14.170714	-0.049910	4.815812
240.075277	8000.490194	14.175719	-0.049940	4.815780
239.736979	8000.576524	14.180723	-0.049877	4.815807
239.927979	8000.583897	14.185728	-0.049913	4.815808
239.866292	8000.577564	14.190733	-0.049901	4.815807
239.817016	8000.595987	14.195738	-0.049892	4.815812
239.718477	8000.564502	14.200743	-0.049874	4.815803
239.714124	8000.569775	14.205747	-0.049873	4.815805
239.811710	8000.499836	14.210752	-0.049891	4.815784
239.846203	8000.559116	14.215757	-0.049898	4.815801
239.864046	8000.420628	14.220762	-0.049901	4.815761
239.688134	8000.593928	14.225767	-0.049869	4.815812
239.772738	8000.565414	14.230771	-0.049884	4.815803
239.866971	8000.577623	14.235776	-0.049902	4.815807
239.916621	8000.573096	14.240781	-0.049911	4.815805
240.133074	8000.576611	14.245786	-0.049952	4.815805
239.899397	8000.479949	14.250791	-0.049908	4.815778
239.857519	8000.562545	14.255795	-0.049900	4.815802
239.922514	7999.512083	14.260800	-0.049912	4.815495

239.783159	7996.216937	14.265805	-0.049884	4.814532
239.912818	7990.658350	14.270810	-0.049904	4.812905
239.971748	7983.952910	14.275815	-0.049911	4.810942
239.681318	7976.612573	14.280819	-0.049852	4.808794
239.498142	7969.025822	14.285824	-0.049813	4.806572
239.549200	7961.201276	14.290829	-0.049818	4.804279
239.574956	7953.359850	14.295834	-0.049818	4.801980
239.459661	7945.436026	14.300839	-0.049791	4.799656
239.395292	7937.423255	14.305843	-0.049774	4.797304
239.599280	7929.445973	14.310848	-0.049807	4.794961
239.305089	7921.361282	14.315853	-0.049747	4.792587
239.416177	7913.384126	14.320858	-0.049762	4.790241
239.315968	7905.401536	14.325863	-0.049738	4.787894
239.230680	7897.392347	14.330867	-0.049717	4.785538
239.213807	7889.425180	14.335872	-0.049709	4.783193
239.128844	7881.435593	14.340877	-0.049688	4.780840
239.124234	7873.400191	14.345882	-0.049682	4.778472
239.056125	7865.415603	14.350887	-0.049664	4.776119
238.880798	7857.390232	14.355891	-0.049626	4.773752
238.934530	7849.392945	14.360896	-0.049631	4.771392
238.943341	7841.377906	14.365901	-0.049628	4.769026
238.715684	7833.400954	14.370906	-0.049580	4.766670
238.777487	7825.335403	14.375911	-0.049587	4.764286
238.642036	7817.384495	14.380915	-0.049556	4.761936
238.622707	7809.370341	14.385920	-0.049548	4.759565
238.547218	7801.413336	14.390925	-0.049528	4.757210
238.925557	7793.368425	14.395930	-0.049594	4.754826
238.534157	7785.354758	14.400935	-0.049516	4.752453
238.448147	7777.260108	14.405939	-0.049494	4.750054
238.510945	7769.292194	14.410944	-0.049501	4.747690
238.519650	7761.307682	14.415949	-0.049497	4.745321
238.370908	7753.313989	14.420954	-0.049465	4.742948
238.457032	7745.358242	14.425959	-0.049475	4.740585
238.166413	7737.293500	14.430963	-0.049416	4.738189
238.077247	7729.374518	14.435968	-0.049394	4.735835
238.142517	7721.306740	14.440973	-0.049401	4.733435
238.276037	7713.312884	14.445978	-0.049421	4.731055
238.056982	7705.288365	14.450983	-0.049375	4.728666
237.888033	7697.289391	14.455987	-0.049339	4.726283
238.100292	7689.329246	14.460992	-0.049373	4.723910
237.972950	7681.329330	14.465997	-0.049344	4.721525
238.020702	7673.296263	14.471002	-0.049348	4.719128
238.054555	7665.394707	14.476007	-0.049349	4.716769
237.631335	7657.303300	14.481011	-0.049265	4.714353
237.697032	7649.293092	14.486016	-0.049272	4.711959
237.596865	7641.246024	14.491021	-0.049248	4.709553
237.682375	7633.308810	14.496026	-0.049259	4.707178
237.599903	7625.296167	14.501031	-0.049239	4.704780
237.429330	7617.304758	14.506035	-0.049202	4.702388
237.596990	7609.339563	14.511040	-0.049228	4.700001
237.489337	7601.343236	14.516045	-0.049202	4.697604
237.326171	7593.271595	14.521050	-0.049167	4.695184
237.281313	7585.313092	14.526055	-0.049153	4.692796
237.393437	7577.204698	14.531059	-0.049169	4.690361
237.149251	7569.316631	14.536064	-0.049119	4.687992
237.075044	7561.270548	14.541069	-0.049100	4.685574
237.250839	7553.301625	14.546074	-0.049127	4.683178
237.175799	7545.313632	14.551079	-0.049108	4.680775
237.081038	7537.264352	14.556083	-0.049085	4.678352
237.126004	7529.353655	14.561088	-0.049088	4.675970
237.025283	7521.195626	14.566093	-0.049064	4.673512
236.787644	7513.143830	14.571098	-0.049015	4.671085
236.854730	7505.238336	14.576103	-0.049022	4.668700
236.854332	7497.196967	14.581107	-0.049017	4.666273
236.665408	7489.194213	14.586112	-0.048977	4.663857
236.653536	7481.250058	14.591117	-0.048970	4.661457
236.819050	7473.232137	14.596122	-0.048995	4.659034
236.660391	7465.317392	14.601127	-0.048961	4.656640
236.232384	7457.208931	14.606131	-0.048876	4.654187
236.283031	7449.261975	14.611136	-0.048880	4.651782
236.274849	7441.199426	14.616141	-0.048873	4.649340
236.554021	7433.215992	14.621146	-0.048920	4.646920
236.519682	7425.216342	14.626151	-0.048908	4.644495
236.501653	7417.242533	14.631155	-0.048900	4.642076
236.477786	7409.252318	14.636160	-0.048890	4.639650
236.324858	7401.279438	14.641165	-0.048857	4.637229
236.427824	7393.182771	14.646170	-0.048871	4.634769
236.288858	7385.202990	14.651175	-0.048840	4.632343
236.073401	7377.153482	14.656179	-0.048794	4.629895
235.991853	7369.228444	14.661184	-0.048774	4.627483
235.941497	7361.156915	14.666189	-0.048760	4.625026
235.862856	7353.202387	14.671194	-0.048740	4.622602
235.766875	7345.179359	14.676199	-0.048717	4.620157
235.851249	7337.192379	14.681203	-0.048727	4.617721
235.894351	7329.215729	14.686208	-0.048730	4.615287
235.631324	7321.149292	14.691213	-0.048676	4.612825
235.786711	7313.127966	14.696218	-0.048700	4.610374
235.876808	7305.182383	14.701223	-0.048711	4.607946
235.717761	7297.161547	14.706227	-0.048677	4.605494
235.682336	7289.210220	14.711232	-0.048665	4.603061
235.638771	7281.219284	14.716237	-0.048652	4.600615
235.509892	7273.186884	14.721242	-0.048623	4.598155
235.546668	7265.213578	14.726247	-0.048624	4.595711
235.394794	7257.126756	14.731251	-0.048591	4.593232
235.517701	7249.088592	14.736256	-0.048608	4.590766
235.225495	7241.110521	14.741261	-0.048549	4.588317
235.221004	7233.131068	14.746266	-0.048543	4.585867
235.194515	7225.186422	14.751271	-0.048533	4.583426
235.044741	7217.128595	14.756275	-0.048500	4.580948
235.011744	7209.157041	14.761280	-0.048489	4.578496
235.156528	7201.133441	14.766285	-0.048510	4.576027
234.957267	7193.164938	14.771290	-0.048468	4.573573
234.781007	7185.121697	14.776295	-0.048430	4.571095
234.737683	7177.106701	14.781299	-0.048417	4.568624
234.868605	7169.143958	14.786304	-0.048436	4.566168
234.679646	7161.121028	14.791309	-0.048396	4.563692
234.484267	7153.151083	14.796314	-0.048354	4.561231
234.668834	7145.168661	14.801319	-0.048383	4.558766
234.584663	7137.184686	14.806323	-0.048363	4.556298
234.475432	7129.190061	14.811328	-0.048337	4.553825
234.397055	7121.130076	14.816333	-0.048317	4.551331
234.491062	7113.092793	14.821338	-0.048330	4.548843
234.413939	7105.131344	14.826343	-0.048310	4.546376
234.365583	7097.094536	14.831347	-0.048296	4.543885
234.429689	7089.142022	14.836352	-0.048303	4.541419
234.453902	7081.090443	14.841357	-0.048302	4.538921
234.159608	7073.185026	14.846362	-0.048242	4.536466
234.207344	7065.149177	14.851367	-0.048246	4.533970
234.137737	7057.098436	14.856371	-0.048228	4.531468
234.020289	7049.093655	14.861376	-0.048201	4.528978
233.844483	7041.137876	14.866381	-0.048163	4.526502
233.924899	7033.091441	14.871386	-0.048173	4.523998
233.787234	7025.159270	14.876391	-0.048142	4.521527
233.821598	7017.104007	14.881395	-0.048143	4.519016
233.935691	7009.203731	14.886400	-0.048159	4.516553
233.778989	7001.081807	14.891405	-0.048125	4.514019
233.765485	6992.975342	14.896410	-0.048117	4.511488
233.908119	6985.027013	14.901415	-0.048139	4.509006
233.757691	6977.058558	14.906419	-0.048106	4.506515
233.789419	6969.053055	14.911424	-0.048106	4.504012
233.600312	6961.094876	14.916429	-0.048066	4.501521
233.518026	6953.081382	14.921434	-0.048045	4.499012
233.475280	6945.125838	14.926439	-0.048032	4.496520
233.287037	6937.055612	14.931443	-0.047992	4.493991
233.460496	6929.058159	14.936448	-0.048019	4.491483
233.244183	6921.021228	14.941453	-0.047974	4.488961
233.126545	6913.040604	14.946458	-0.047947	4.486455
233.177003	6905.095550	14.951463	-0.047951	4.483960
233.143567	6897.107127	14.956467	-0.047940	4.481449
233.115532	6889.065576	14.961472	-0.047929	4.478920
232.919359	6881.097871	14.966477	-0.047888	4.476413
233.294111	6873.037179	14.971482	-0.047952	4.473876
233.051319	6865.050305	14.976487	-0.047902	4.471360
232.658150	6857.003406	14.981491	-0.047823	4.468822
232.785453	6849.049196	14.986496	-0.047842	4.466314
232.668743	6841.028116	14.991501	-0.047815	4.463783
232.538327	6833.030589	14.996506	-0.047786	4.461258
232.708279	6825.069542	15.001511	-0.047812	4.458743
232.617031	6817.049026	15.006515	-0.047790	4.456208
232.626152	6809.027903	15.011520	-0.047787	4.453671
232.633786	6800.997564	15.016525	-0.047783	4.451130
232.605148	6792.963417	15.021530	-0.047772	4.448587
232.394685	6785.066336	15.026535	-0.047728	4.446084
232.177839	6777.009439	15.031539	-0.047683	4.443529
232.507791	6769.031513	15.036544	-0.047739	4.441000
232.216080	6761.039044	15.041549	-0.047679	4.438463
232.281622	6753.020715	15.046554	-0.047686	4.435917
232.350031	6744.984336	15.051559	-0.047694	4.433364
232.051483	6736.924459	15.056563	-0.047633	4.430801
232.118379	6728.998482	15.061568	-0.047641	4.428280
232.098500	6720.961577	15.066573	-0.047632	4.425722
232.080591	6712.991053	15.071578	-0.047623	4.423184
232.158600	6705.010932	15.076583	-0.047633	4.420642
231.903716	6697.020905	15.081587	-0.047580	4.418093
231.816920	6689.031029	15.086592	-0.047559	4.415544
231.974810	6681.005780	15.091597	-0.047583	4.412984
231.657291	6672.969249	15.096602	-0.047519	4.410415
231.813642	6664.994360	15.101607	-0.047543	4.407868
231.681269	6656.904765	15.106611	-0.047513	4.405281
231.732150	6649.003295	15.111616	-0.047517	4.402753
231.400962	6641.024976	15.116621	-0.047450	4.400197
231.476074	6633.027030	15.121626	-0.047459	4.397636
231.396039	6625.036372	15.126631	-0.047439	4.395075
231.392440	6616.981933	15.131635	-0.047433	4.392492
231.334157	6608.959460	15.136640	-0.047417	4.389918
231.392384	6600.995079	15.141645	-0.047423	4.387361
231.148659	6592.975622	15.146650	-0.047372	4.384784
231.160122	6585.026290	15.151655	-0.047369	4.382228
231.190511	6576.954125	15.156659	-0.047370	4.379633
231.270395	6569.014822	15.161664	-0.047380	4.377078
231.026491	6561.016372	15.166669	-0.047329	4.374501
230.994020	6552.999386	15.171674	-0.047318	4.371918
231.004726	6544.966974	15.176679	-0.047315	4.369329
230.660986	6537.011934	15.181683	-0.047246	4.366761
230.754567	6528.999078	15.186688	-0.047258	4.364175
230.667313	6521.072767	15.191693	-0.047236	4.361615
230.586362	6512.984901	15.196698	-0.047216	4.359000
230.612147	6505.067750	15.201703	-0.047216	4.356441
230.508905	6496.963950	15.206707	-0.047191	4.353818
230.408968	6488.903579	15.211712	-0.047168	4.351208
230.434870	6480.915842	15.216717	-0.047167	4.348621
230.359546	6472.941698	15.221722	-0.047148	4.346036
230.476399	6464.949061	15.226727	-0.047165	4.343445
230.354623	6456.975821	15.231731	-0.047137	4.340857
230.390726	6448.992487	15.236736	-0.047138	4.338265
230.262200	6440.979038	15.241741	-0.047109	4.335660
230.236979	6432.919254	15.246746	-0.047100	4.333040
230.006131	6424.940834	15.251751	-0.047051	4.330443
230.102851	6416.966767	15.256755	-0.047064	4.327848
229.917375	6408.951997	15.261760	-0.047025	4.325237
230.053827	6401.025891	15.266765	-0.047045	4.322655
229.857455	6392.995253	15.271770	-0.047003	4.320035
229.877084	6385.018198	15.276775	-0.047002	4.317433
229.571169	6376.959780	15.281779	-0.046939	4.314799
229.731475	6368.925174	15.286784	-0.046964	4.312176
229.668840	6360.911139	15.291789	-0.046947	4.309556
229.785588	6352.911124	15.296794	-0.046964	4.306940
229.659839	6344.942698	15.301799	-0.046935	4.304332
229.441375	6336.973766	15.306803	-0.046890	4.301720
229.488293	6328.947134	15.311808	-0.046893	4.299091
229.341040	6320.999640	15.316813	-0.046861	4.296484
229.341033	6312.951613	15.321818	-0.046855	4.293844
229.330346	6304.901204	15.326823	-0.046848	4.291201
229.234366	6296.893057	15.331827	-0.046825	4.288570
229.208471	6288.950777	15.336832	-0.046815	4.285959
229.105443	6280.920413	15.341837	-0.046791	4.283317
229.118035	6272.932875	15.346842	-0.046788	4.280689
229.182265	6264.952704	15.351847	-0.046795	4.278062
229.099978	6256.939546	15.356851	-0.046774	4.275421
229.180224	6248.904404	15.361856	-0.046784	4.272772
229.092689	6240.886215	15.366861	-0.046763	4.270126
229.019798	6232.890613	15.371866	-0.046744	4.267486
229.085011	6224.884015	15.376871	-0.046751	4.264842
228.846255	6216.941552	15.381875	-0.046701	4.262215
228.689708	6208.887667	15.386880	-0.046667	4.259550
228.742471	6200.935028	15.391885	-0.046672	4.256919
228.845990	6192.874673	15.396890	-0.046686	4.254251
228.727074	6184.937603	15.401895	-0.046659	4.251620
228.750204	6176.881038	15.406899	-0.046658	4.248949
228.596222	6168.932359	15.411904	-0.046624	4.246311
228.464409	6160.922250	15.416909	-0.046594	4.243651
228.331029	6152.963309	15.421914	-0.046564	4.241006
228.549989	6144.959843	15.426919	-0.046600	4.238348
228.326613	6136.964715	15.431923	-0.046553	4.235686
228.151368	6128.923605	15.436928	-0.046515	4.233009
228.205857	6120.911863	15.441933	-0.046520	4.230341
228.171796	6112.937742	15.446938	-0.046509	4.227684
228.271571	6104.929116	15.451943	-0.046522	4.225014
228.353679	6096.953174	15.456947	-0.046532	4.222354
228.227383	6088.946428	15.461952	-0.046504	4.219680
228.122456	6081.009569	15.466957	-0.046479	4.217027
227.887231	6072.904324	15.471962	-0.046430	4.214316
228.002721	6064.979333	15.476967	-0.046446	4.211666
227.839192	6056.936414	15.481971	-0.046411	4.208972
227.703124	6048.951915	15.486976	-0.046380	4.206297
227.709995	6040.952264	15.491981	-0.046377	4.203616
227.848781	6032.913559	15.496986	-0.046397	4.200922
227.775255	6024.987121	15.501991	-0.046378	4.198261
227.549276	6016.957195	15.506995	-0.046331	4.195562
227.713389	6008.875469	15.512000	-0.046356	4.192849
227.687663	6000.870005	15.517005	-0.046347	4.190157
227.261976	5992.884511	15.522010	-0.046262	4.187466
227.249162	5984.925184	15.527015	-0.046255	4.184786
227.217203	5976.949360	15.532019	-0.046244	4.182099
227.218948	5968.939609	15.537024	-0.046239	4.179399
227.279587	5960.959922	15.542029	-0.046245	4.176708
227.361487	5952.856119	15.547034	-0.046255	4.173974
227.378194	5944.905792	15.552039	-0.046253	4.171289
226.983881	5936.931047	15.557043	-0.046174	4.168589
227.104844	5928.894317	15.562048	-0.046192	4.165873
227.018445	5920.948258	15.567053	-0.046170	4.163183
226.913466	5912.928749	15.572058	-0.046146	4.160466
226.895221	5904.949300	15.577063	-0.046137	4.157762
226.733412	5896.909163	15.582067	-0.046102	4.155034
226.676643	5888.888192	15.587072	-0.046086	4.152312
226.666068	5880.850666	15.592077	-0.046079	4.149583
226.503423	5872.884437	15.597082	-0.046044	4.146875
226.506760	5864.913925	15.602087	-0.046039	4.144165
226.383057	5856.944906	15.607091	-0.046011	4.141453
226.470634	5848.933248	15.612096	-0.046022	4.138727
226.439616	5840.943027	15.617101	-0.046011	4.136005
226.253471	5832.909688	15.622106	-0.045971	4.133264
226.264163	5824.880992	15.627111	-0.045968	4.130526
226.322150	5816.880579	15.632115	-0.045974	4.127796
226.393948	5808.901383	15.637120	-0.045982	4.125072
226.212953	5800.953233	15.642125	-0.045943	4.122353
226.175110	5792.891918	15.647130	-0.045931	4.119596
226.290210	5784.966187	15.652135	-0.045947	4.116885
226.065183	5776.926276	15.657139	-0.045900	4.114129
226.087451	5768.868844	15.662144	-0.045899	4.111368
225.912559	5760.868912	15.667149	-0.045861	4.108623
225.814264	5752.886033	15.672154	-0.045838	4.105882
225.920415	5744.919773	15.677159	-0.045853	4.103148
225.945431	5736.915590	15.682163	-0.045852	4.100398
225.574988	5728.977491	15.687168	-0.045778	4.097664
225.530056	5720.957786	15.692173	-0.045764	4.094904
225.701988	5712.902388	15.697178	-0.045791	4.092133
225.778770	5704.921350	15.702183	-0.045800	4.089385
225.531367	5696.942178	15.707187	-0.045749	4.086630
225.488714	5688.937742	15.712192	-0.045736	4.083868
225.585271	5680.980197	15.717197	-0.045749	4.081123
225.324555	5672.957388	15.722202	-0.045695	4.078347
225.458757	5664.985625	15.727207	-0.045715	4.075593
225.247355	5656.930351	15.732211	-0.045671	4.072804
225.283641	5648.917492	15.737216	-0.045672	4.070031
225.416840	5640.962883	15.742221	-0.045692	4.067277
225.180469	5632.915355	15.747226	-0.045643	4.064484
225.324986	5624.998097	15.752231	-0.045665	4.061740
225.111593	5616.965215	15.757235	-0.045620	4.058949
225.048481	5608.967632	15.762240	-0.045603	4.056170
225.002032	5600.939849	15.767245	-0.045589	4.053379
224.823255	5592.912421	15.772250	-0.045550	4.050584
224.840579	5584.935230	15.777255	-0.045549	4.047807
224.801852	5576.954243	15.782259	-0.045536	4.045027
224.848042	5568.985891	15.787264	-0.045540	4.042250
224.600364	5560.935374	15.792269	-0.045488	4.039438
224.499216	5552.981730	15.797274	-0.045464	4.036661
224.694679	5544.932332	15.802279	-0.045496	4.033852
224.498241	5536.823332	15.807283	-0.045454	4.031015
224.364128	5528.894083	15.812288	-0.045424	4.028240
224.489433	5520.904608	15.817293	-0.045442	4.025445
224.394989	5512.921392	15.822298	-0.045419	4.022647
224.283720	5504.940069	15.827303	-0.045393	4.019848
224.293886	5496.957189	15.832307	-0.045390	4.017048
224.338682	5488.945435	15.837312	-0.045393	4.014237
224.242908	5480.938466	15.842317	-0.045370	4.011423
224.153828	5472.919992	15.847322	-0.045348	4.008603
224.229351	5464.916630	15.852327	-0.045357	4.005790
224.028771	5456.920747	15.857331	-0.045315	4.002972
224.010652	5448.927593	15.862336	-0.045306	4.000156
223.884784	5440.970685	15.867341	-0.045278	3.997350
223.808753	5432.921581	15.872346	-0.045258	3.994509
223.930500	5424.923051	15.877351	-0.045276	3.991688
223.876147	5416.915317	15.882355	-0.045261	3.988858
223.625098	5408.937453	15.887360	-0.045209	3.986034
223.601423	5400.960029	15.892365	-0.045199	3.983212
223.404504	5392.928516	15.897370	-0.045157	3.980366
223.546116	5384.980281	15.902375	-0.045179	3.977552
223.287457	5376.953539	15.907379	-0.045125	3.974703
223.394202	5368.952271	15.912384	-0.045140	3.971866
223.436770	5360.933366	15.917389	-0.045143	3.969020
223.163713	5352.948487	15.922394	-0.045087	3.966179
223.202813	5344.992198	15.927399	-0.045089	3.963351
223.238608	5336.984717	15.932403	-0.045091	3.960502
223.126344	5329.018213	15.937408	-0.045064	3.957664
223.132493	5321.022811	15.942413	-0.045060	3.954816
223.021139	5312.946128	15.947418	-0.045035	3.951934
223.077522	5304.954635	15.952423	-0.045040	3.949084
222.907379	5296.982666	15.957427	-0.045003	3.946234
222.845274	5288.951803	15.962432	-0.044986	3.943364
222.929439	5280.994624	15.967437	-0.044997	3.940520
222.924891	5272.986529	15.972442	-0.044991	3.937654
222.791453	5265.014246	15.977447	-0.044961	3.934797
222.735797	5256.982082	15.982451	-0.044945	3.931917
222.798277	5248.962934	15.987456	-0.044952	3.929043
222.644416	5241.054493	15.992461	-0.044918	3.926202
222.366267	5233.019993	15.997466	-0.044861	3.923311
222.519399	5225.036421	16.002471	-0.044884	3.920444
222.310491	5217.069340	16.007475	-0.044840	3.917575
222.272288	5209.013591	16.012480	-0.044828	3.914675
222.332192	5201.034154	16.017485	-0.044834	3.911801
222.248556	5192.964963	16.022490	-0.044813	3.908891
222.139441	5185.004364	16.027495	-0.044788	3.906017
222.061731	5176.993579	16.032499	-0.044768	3.903124
222.325375	5169.000286	16.037504	-0.044812	3.900241
222.060806	5161.060386	16.042509	-0.044758	3.897365
222.067935	5153.009504	16.047514	-0.044754	3.894452
222.201317	5145.017441	16.052519	-0.044774	3.891561
222.263705	5136.972166	16.057523	-0.044780	3.888647
221.896614	5129.019469	16.062528	-0.044707	3.885756
221.801851	5121.067751	16.067533	-0.044684	3.882868
221.934547	5113.024715	16.072538	-0.044703	3.879950
221.712370	5105.106401	16.077543	-0.044657	3.877068
221.508861	5096.996579	16.082547	-0.044614	3.874114
221.512247	5088.757497	16.087552	-0.044609	3.871115
221.680666	5080.852501	16.092557	-0.044635	3.868239
221.342679	5072.900519	16.097562	-0.044567	3.865333
221.485517	5064.983904	16.102567	-0.044589	3.862448
221.352096	5056.961845	16.107571	-0.044559	3.859516
221.275516	5048.994908	16.112576	-0.044539	3.856604
221.404930	5040.998716	16.117581	-0.044558	3.853682
221.415783	5033.006603	16.122586	-0.044555	3.850758
221.321298	5025.050302	16.127591	-0.044533	3.847842
221.092499	5017.010524	16.132595	-0.044485	3.844891
221.083737	5009.068468	16.137600	-0.044478	3.841978
221.056967	5001.062042	16.142605	-0.044468	3.839039
220.749722	4993.114165	16.147610	-0.044406	3.836113
220.834420	4985.072141	16.152615	-0.044416	3.833158
220.909769	4977.013917	16.157619	-0.044425	3.830195
220.874910	4969.050419	16.162624	-0.044413	3.827262
220.531845	4961.089548	16.167629	-0.044344	3.824322
220.581786	4953.119957	16.172634	-0.044349	3.821384
220.428733	4945.092936	16.177639	-0.044315	3.818418
220.413013	4937.110744	16.182643	-0.044307	3.815470
220.441135	4929.079838	16.187648	-0.044307	3.812502
220.518136	4921.096200	16.192653	-0.044316	3.809550
220.537840	4913.090041	16.197658	-0.044315	3.806587
220.474843	4905.126978	16.202663	-0.044298	3.803635
220.388028	4897.127764	16.207667	-0.044276	3.800668
220.258867	4889.153324	16.212672	-0.044247	3.797706
220.188660	4881.139653	16.217677	-0.044229	3.794728
220.204692	4873.067561	16.222682	-0.044227	3.791729
220.313990	4865.070127	16.227687	-0.044242	3.788757
220.203493	4857.085377	16.232691	-0.044216	3.785782
220.109771	4849.098410	16.237696	-0.044194	3.782805
220.056525	4841.133755	16.242701	-0.044179	3.779834
219.901660	4833.130513	16.247706	-0.044145	3.776844
219.865822	4825.147357	16.252711	-0.044133	3.773862
219.827410	4817.091357	16.257715	-0.044120	3.770851
219.517444	4809.112623	16.262720	-0.044058	3.767860
219.587875	4801.112078	16.267725	-0.044066	3.764867
219.628173	4793.120554	16.272730	-0.044068	3.761874
219.739948	4785.149288	16.277735	-0.044084	3.758888
219.526314	4777.155348	16.282739	-0.044039	3.755884
219.415883	4769.106657	16.287744	-0.044013	3.752859
219.485641	4761.096485	16.292749	-0.044021	3.749850
219.498129	4753.101269	16.297754	-0.044018	3.746843
219.528676	4745.126265	16.302759	-0.044019	3.743842
219.479356	4737.147750	16.307763	-0.044004	3.740835
219.234091	4729.186357	16.312768	-0.043953	3.737828
219.279320	4721.193292	16.317773	-0.043957	3.734813
219.095526	4713.146798	16.322778	-0.043917	3.731770
219.108813	4705.155536	16.327783	-0.043915	3.728750
218.876156	4697.184772	16.332787	-0.043866	3.725730
218.900809	4689.164563	16.337792	-0.043866	3.722694
219.063723	4681.193095	16.342797	-0.043891	3.719678
218.848665	4673.231758	16.347802	-0.043846	3.716654
218.789719	4665.219235	16.352807	-0.043829	3.713612
218.632644	4657.098873	16.357811	-0.043795	3.710524
218.673809	4649.144068	16.362816	-0.043798	3.707501
218.698703	4641.167267	16.367821	-0.043797	3.704467
218.609639	4633.181484	16.372826	-0.043775	3.701425
218.695980	4625.208846	16.377831	-0.043786	3.698389
218.618365	4617.230576	16.382835	-0.043767	3.695344
218.455005	4609.229411	16.387840	-0.043731	3.692286
218.304857	4601.233262	16.392845	-0.043698	3.689228
218.361480	4593.240731	16.397850	-0.043703	3.686174
218.268552	4585.273712	16.402855	-0.043681	3.683123
217.941449	4577.273531	16.407859	-0.043615	3.680051
217.950608	4569.286208	16.412864	-0.043611	3.676990
217.809343	4561.282265	16.417869	-0.043580	3.673916
217.738921	4553.225054	16.422874	-0.043562	3.670820
218.053262	4545.223461	16.427879	-0.043615	3.667754
217.809011	4537.241840	16.432883	-0.043564	3.664678
217.884955	4529.260734	16.437888	-0.043573	3.661608
218.034429	4521.282104	16.442893	-0.043596	3.658539
217.874615	4513.270489	16.447898	-0.043561	3.655446
217.736794	4505.277976	16.452903	-0.043530	3.652358
217.600664	4497.259042	16.457907	-0.043500	3.649258
217.607103	4489.292896	16.462912	-0.043496	3.646179
217.614420	4481.293087	16.467917	-0.043492	3.643084
217.629850	4473.318055	16.472922	-0.043490	3.639997
217.552512	4465.380379	16.477927	-0.043470	3.636919
217.537453	4457.313978	16.482931	-0.043462	3.633790
217.218964	4449.262831	16.487936	-0.043398	3.630656
217.208530	4441.289617	16.492941	-0.043391	3.627558
217.041689	4433.272395	16.497946	-0.043355	3.624436
216.980887	4425.348522	16.502951	-0.043338	3.621351
217.092740	4417.324727	16.507955	-0.043354	3.618228
217.163172	4409.331553	16.512960	-0.043362	3.615114
217.089773	4401.353837	16.517965	-0.043343	3.611999
216.824388	4393.332759	16.522970	-0.043288	3.608860
216.901207	4385.355874	16.527975	-0.043298	3.605744
216.868889	4377.377700	16.532979	-0.043286	3.602622
216.744095	4369.390772	16.537984	-0.043258	3.599491
216.946998	4361.423941	16.542989	-0.043291	3.596375
216.931369	4353.370673	16.547994	-0.043283	3.593216
216.662367	4345.387318	16.552999	-0.043227	3.590074
216.540077	4337.403629	16.558003	-0.043199	3.586934
216.481080	4329.412874	16.563008	-0.043183	3.583789
216.262606	4321.447118	16.568013	-0.043137	3.580648
216.087322	4313.439361	16.573018	-0.043100	3.577488
216.291766	4305.451329	16.578023	-0.043133	3.574344
216.323875	4297.426745	16.583027	-0.043133	3.571178
216.246303	4289.406281	16.588032	-0.043114	3.568008
216.335769	4281.439070	16.593037	-0.043125	3.564860
216.093443	4273.468705	16.598042	-0.043075	3.561699
215.949045	4265.469115	16.603047	-0.043043	3.558527
215.974555	4257.443629	16.608051	-0.043043	3.555346
215.914614	4249.363264	16.613056	-0.043026	3.552138
216.115165	4241.379983	16.618061	-0.043058	3.548974
215.734636	4233.359357	16.623066	-0.042982	3.545774
215.835341	4225.466863	16.628071	-0.042996	3.542637
215.634612	4217.453561	16.633075	-0.042954	3.539440
215.658649	4209.459591	16.638080	-0.042953	3.536255
215.651912	4201.455591	16.643085	-0.042946	3.533062
215.539972	4193.433997	16.648090	-0.042920	3.529855
215.560515	4185.487748	16.653095	-0.042919	3.526680
215.323746	4177.479350	16.658099	-0.042870	3.523470
215.366467	4169.499073	16.663104	-0.042873	3.520276
215.354686	4161.544221	16.668109	-0.042865	3.517088
215.168687	4153.506513	16.673114	-0.042826	3.513858
215.128990	4145.488328	16.678119	-0.042813	3.510638
215.355266	4137.505120	16.683123	-0.042850	3.507437
215.152250	4129.494079	16.688128	-0.042807	3.504208
215.051460	4121.602726	16.693133	-0.042783	3.501028
215.123928	4113.551771	16.698138	-0.042792	3.497786
215.040805	4105.575327	16.703143	-0.042771	3.494567
214.990058	4097.570506	16.708147	-0.042756	3.491333
214.938755	4089.574716	16.713152	-0.042742	3.488101
214.870778	4081.582277	16.718157	-0.042724	3.484866
214.547638	4073.639758	16.723162	-0.042659	3.481641
214.573496	4065.634826	16.728167	-0.042658	3.478398
214.578705	4057.645911	16.733171	-0.042654	3.475158
214.387127	4049.607818	16.738176	-0.042613	3.471888
214.674352	4041.599184	16.743181	-0.042661	3.468643
214.509731	4033.606344	16.748186	-0.042626	3.465387
214.269948	4025.643204	16.753191	-0.042576	3.462137
214.367911	4017.658285	16.758195	-0.042589	3.458887
214.209365	4009.673902	16.763200	-0.042554	3.455625
214.476897	4001.662815	16.768205	-0.042599	3.452363
214.166952	3993.617993	16.773210	-0.042536	3.449065
213.906974	3985.683772	16.778215	-0.042483	3.445811
214.091468	3977.684529	16.783219	-0.042512	3.442542
214.075788	3969.653497	16.788224	-0.042504	3.439250
214.013266	3961.734397	16.793229	-0.042487	3.436000
214.018938	3953.680457	16.798234	-0.042483	3.432693
213.779664	3945.699137	16.803239	-0.042433	3.429404
213.837135	3937.733842	16.808243	-0.042439	3.426129
213.695562	3929.697799	16.813248	-0.042407	3.422815
213.781594	3921.738653	16.818253	-0.042418	3.419538
213.724490	3913.753557	16.823258	-0.042402	3.416241
213.678574	3905.749583	16.828263	-0.042389	3.412934
213.772730	3897.733456	16.833267	-0.042401	3.409623
213.494872	3889.787719	16.838272	-0.042344	3.406326
213.468554	3881.824300	16.843277	-0.042334	3.403027
213.411282	3873.782398	16.848282	-0.042318	3.399690
213.512889	3865.838113	16.853287	-0.042332	3.396397
213.614015	3857.758057	16.858291	-0.042346	3.393044
213.477254	3849.705979	16.863296	-0.042315	3.389691
213.377076	3841.793044	16.868301	-0.042291	3.386394
213.220735	3833.803492	16.873306	-0.042257	3.383060
213.237676	3825.823661	16.878311	-0.042255	3.379732
213.242911	3817.849691	16.883315	-0.042251	3.376403
213.079597	3809.846419	16.888320	-0.042215	3.373053
213.037598	3801.849775	16.893325	-0.042202	3.369707
212.935842	3793.878880	16.898330	-0.042178	3.366366
212.951731	3785.862681	16.903335	-0.042176	3.363006
212.702728	3777.906265	16.908339	-0.042125	3.359659
212.415227	3769.935210	16.913344	-0.042066	3.356301
212.598596	3761.916771	16.918349	-0.042095	3.352937
212.447387	3753.879638	16.923354	-0.042062	3.349549
212.565782	3745.899182	16.928359	-0.042078	3.346192
212.456193	3737.905800	16.933363	-0.042053	3.342817
212.265581	3729.920951	16.938368	-0.042012	3.339440
212.444604	3721.984377	16.943373	-0.042040	3.336093
212.373625	3713.951403	16.948378	-0.042022	3.332693
212.189863	3705.952033	16.953383	-0.041983	3.329299
212.059616	3697.995965	16.958387	-0.041953	3.325923
212.146899	3689.982546	16.963392	-0.041964	3.322526
212.138427	3681.998961	16.968397	-0.041958	3.319135
211.832055	3674.063845	16.973402	-0.041896	3.315750
211.828963	3666.021368	16.978407	-0.041890	3.312328
211.782118	3658.005747	16.983411	-0.041876	3.308911
211.914615	3649.993436	16.988416	-0.041895	3.305500
211.908851	3642.055770	16.993421	-0.041889	3.302111
211.634085	3634.057578	16.998426	-0.041833	3.298683
211.759698	3626.080824	17.003431	-0.041851	3.295275
211.597632	3618.087824	17.008435	-0.041816	3.291846
211.425919	3610.074257	17.013440	-0.041779	3.288405
211.586303	3602.095928	17.018445	-0.041803	3.284987
211.343195	3594.150681	17.023450	-0.041753	3.281565
211.423339	3586.137391	17.028455	-0.041763	3.278122
211.471704	3578.165089	17.033459	-0.041767	3.274693
211.438223	3570.144843	17.038464	-0.041755	3.271235
211.135228	3562.172860	17.043469	-0.041694	3.267785
211.144648	3554.125985	17.048474	-0.041690	3.264310
211.201473	3546.162016	17.053479	-0.041696	3.260870
211.061265	3538.196384	17.058483	-0.041664	3.257417
210.905645	3530.206833	17.063488	-0.041630	3.253950
210.985105	3522.194143	17.068493	-0.041640	3.250478
210.887132	3514.182643	17.073498	-0.041617	3.246996
210.758837	3506.234288	17.078503	-0.041588	3.243537
210.719236	3498.259717	17.083507	-0.041575	3.240066
210.605847	3490.274063	17.088512	-0.041549	3.236583
210.505130	3482.279423	17.093517	-0.041525	3.233093
210.416010	3474.223756	17.098522	-0.041503	3.229573
210.504564	3466.228861	17.103527	-0.041514	3.226084
210.542902	3458.250848	17.108531	-0.041516	3.222595
210.299560	3450.286525	17.113536	-0.041466	3.219098
210.349800	3442.332545	17.118541	-0.041470	3.215613
210.155676	3434.325591	17.123546	-0.041429	3.212091
210.092800	3426.309439	17.128551	-0.041412	3.208567
210.050008	3418.325767	17.133555	-0.041399	3.205054
210.027134	3410.355362	17.138560	-0.041390	3.201543
210.066608	3402.411856	17.143565	-0.041392	3.198043
209.837758	3394.401466	17.148570	-0.041344	3.194499
209.994558	3386.376702	17.153575	-0.041368	3.190961
209.957745	3378.399032	17.158579	-0.041356	3.187431
209.772701	3370.399320	17.163584	-0.041316	3.183881
209.724434	3362.430690	17.168589	-0.041302	3.180347
209.723113	3354.458693	17.173594	-0.041297	3.176809
209.556095	3346.469408	17.178599	-0.041261	3.173253
209.605600	3338.448608	17.183603	-0.041265	3.169688
209.592947	3330.461748	17.188608	-0.041257	3.166132
209.395081	3322.524931	17.193613	-0.041215	3.162585
209.370192	3314.523673	17.198618	-0.041206	3.159014
209.542824	3306.552759	17.203623	-0.041233	3.155460
209.464361	3298.517565	17.208627	-0.041213	3.151863
209.406671	3290.520216	17.213632	-0.041197	3.148280
209.317035	3282.529565	17.218637	-0.041175	3.144694
209.274378	3274.571275	17.223642	-0.041162	3.141120
209.024057	3266.591094	17.228647	-0.041110	3.137524
208.975627	3258.620417	17.233651	-0.041096	3.133936
209.014056	3250.567870	17.238656	-0.041098	3.130312
208.970128	3242.639356	17.243661	-0.041085	3.126735
208.839818	3234.649002	17.248666	-0.041055	3.123123
208.832339	3226.655075	17.253671	-0.041049	3.119510
208.764511	3218.706073	17.258675	-0.041031	3.115910
208.713814	3210.668146	17.263680	-0.041016	3.112267
208.687202	3202.691609	17.268685	-0.041006	3.108649
208.676192	3194.673332	17.273690	-0.040999	3.105008
208.673566	3186.718542	17.278695	-0.040994	3.101392
208.435165	3178.761062	17.283699	-0.040944	3.097760
208.626764	3170.726619	17.288704	-0.040975	3.094108
208.374345	3162.769595	17.293709	-0.040922	3.090467
208.235906	3154.777769	17.298714	-0.040891	3.086811
208.081277	3146.797123	17.303719	-0.040858	3.083155
208.345863	3138.800551	17.308723	-0.040902	3.079506
208.242763	3130.850682	17.313728	-0.040877	3.075858
208.308592	3122.802668	17.318733	-0.040884	3.072168
208.069816	3114.776342	17.323738	-0.040835	3.068469
207.803793	3106.810085	17.328743	-0.040780	3.064793
207.883000	3098.862219	17.333747	-0.040790	3.061136
207.929055	3090.850068	17.338752	-0.040793	3.057444
207.970330	3082.875100	17.343757	-0.040796	3.053764
207.524055	3074.907267	17.348762	-0.040707	3.050060
207.600015	3066.951436	17.353767	-0.040716	3.046382
207.569539	3058.967016	17.358771	-0.040706	3.042682
207.528626	3050.970540	17.363776	-0.040693	3.038970
207.518547	3043.008200	17.368781	-0.040686	3.035272
207.342075	3034.995705	17.373786	-0.040648	3.031537
207.203355	3026.997956	17.378791	-0.040617	3.027807
207.233389	3019.034701	17.383795	-0.040617	3.024096
207.075658	3011.068073	17.388800	-0.040583	3.020370
207.316251	3003.081675	17.393805	-0.040623	3.016649
207.127962	2995.073306	17.398810	-0.040582	3.012893
206.989184	2987.077148	17.403815	-0.040551	3.009140
207.092878	2979.116729	17.408819	-0.040565	3.005411
206.806394	2971.154142	17.413824	-0.040507	3.001657
206.879690	2963.180903	17.418829	-0.040516	2.997911
206.689262	2955.188519	17.423834	-0.040475	2.994139
206.725658	2947.159093	17.428839	-0.040477	2.990355
206.672662	2939.186984	17.433843	-0.040462	2.986589
206.422624	2931.208302	17.438848	-0.040410	2.982806
206.540892	2923.249393	17.443853	-0.040427	2.979045
206.422398	2915.262550	17.448858	-0.040400	2.975255
206.571780	2907.238871	17.453863	-0.040422	2.971456
206.594522	2899.252087	17.458867	-0.040421	2.967663
206.317161	2891.295270	17.463872	-0.040364	2.963864
206.176138	2883.341993	17.468877	-0.040333	2.960069
206.321973	2875.343867	17.473882	-0.040355	2.956262
206.403584	2867.345259	17.478887	-0.040365	2.952447
206.154626	2859.368559	17.483891	-0.040314	2.948620
206.107180	2851.367477	17.488896	-0.040300	2.944787
206.188481	2843.420138	17.493901	-0.040310	2.940982
205.865735	2835.454828	17.498906	-0.040244	2.937142
205.857035	2827.439281	17.503911	-0.040238	2.933289
205.867919	2819.445747	17.508915	-0.040235	2.929443
205.636199	2811.487934	17.513920	-0.040186	2.925596
205.876144	2803.499402	17.518925	-0.040226	2.921754
205.626312	2795.555611	17.523930	-0.040174	2.917903
205.588304	2787.563693	17.528935	-0.040162	2.914034
205.415270	2779.504535	17.533939	-0.040125	2.910121
205.455511	2771.506751	17.538944	-0.040127	2.906243
205.401874	2763.564034	17.543949	-0.040112	2.902382
205.233543	2755.594576	17.548954	-0.040075	2.898497
205.183718	2747.618271	17.553959	-0.040061	2.894609
205.408975	2739.593372	17.558963	-0.040098	2.890708
205.263983	2731.632515	17.563968	-0.040066	2.886812
205.144888	2723.675130	17.568973	-0.040038	2.882914
205.080113	2715.711039	17.573978	-0.040021	2.879011
205.104563	2707.737625	17.578983	-0.040020	2.875102
205.022435	2699.757752	17.583987	-0.040000	2.871180
204.905520	2691.750221	17.588992	-0.039973	2.867236
205.046863	2683.781767	17.593997	-0.039994	2.863320
204.881848	2675.804214	17.599002	-0.039958	2.859378
204.749884	2667.844767	17.604007	-0.039929	2.855441
204.862495	2659.859271	17.609011	-0.039945	2.851499
204.710275	2651.852344	17.614016	-0.039911	2.847526
204.485980	2643.925255	17.619021	-0.039864	2.843583
204.667667	2635.923587	17.624026	-0.039893	2.839621
204.613088	2627.969279	17.629031	-0.039878	2.835663
204.446637	2619.964285	17.634035	-0.039841	2.831668
204.132002	2611.979458	17.639040	-0.039778	2.827669
204.334150	2603.985126	17.644045	-0.039810	2.823689
204.176916	2596.011292	17.649050	-0.039776	2.819694
204.099186	2588.062156	17.654055	-0.039756	2.815709
203.897997	2580.075660	17.659059	-0.039714	2.811693
203.792223	2572.077276	17.664064	-0.039689	2.807670
203.752993	2564.139197	17.669069	-0.039676	2.803676
203.743634	2556.154481	17.674074	-0.039669	2.799655
203.881352	2548.169795	17.679079	-0.039690	2.795636
203.699962	2540.185308	17.684083	-0.039651	2.791593
203.619911	2532.210593	17.689088	-0.039631	2.787555
203.542894	2524.237270	17.694093	-0.039611	2.783512
203.466324	2516.260144	17.699098	-0.039592	2.779461
203.431358	2508.293520	17.704103	-0.039580	2.775413
203.324071	2500.293638	17.709107	-0.039555	2.771336
203.344190	2492.292510	17.714112	-0.039554	2.767261
203.425278	2484.342477	17.719117	-0.039564	2.763210
203.327538	2476.384150	17.724122	-0.039541	2.759138
203.051185	2468.450097	17.729127	-0.039484	2.755061
203.133945	2460.355368	17.734131	-0.039494	2.750917
202.806333	2452.380776	17.739136	-0.039428	2.746804
203.002793	2444.409774	17.744141	-0.039460	2.742719
203.174052	2436.423222	17.749146	-0.039486	2.738618
202.934472	2428.488175	17.754151	-0.039437	2.734512
202.698216	2420.531555	17.759155	-0.039387	2.730389
202.687564	2412.545767	17.764160	-0.039380	2.726259
202.720706	2404.596381	17.769165	-0.039381	2.722144
202.686301	2396.608118	17.774170	-0.039370	2.717998
202.721659	2388.620718	17.779175	-0.039371	2.713851
202.706898	2380.637716	17.784179	-0.039363	2.709696
202.469177	2372.669157	17.789184	-0.039314	2.705529
202.439717	2364.735213	17.794189	-0.039303	2.701386
202.318813	2356.752241	17.799194	-0.039276	2.697206
202.260424	2348.771198	17.804199	-0.039260	2.693024
202.045283	2340.803655	17.809203	-0.039214	2.688833
202.131941	2332.803855	17.814208	-0.039225	2.684637
201.761858	2324.890198	17.819213	-0.039151	2.680451
201.856093	2316.903786	17.824218	-0.039164	2.676250
201.896531	2308.898553	17.829223	-0.039166	2.672029
201.890064	2300.922277	17.834227	-0.039160	2.667813
201.844926	2292.916762	17.839232	-0.039146	2.663573
201.709669	2284.977382	17.844237	-0.039116	2.659355
201.727048	2277.010866	17.849242	-0.039114	2.655126
201.631864	2269.018316	17.854247	-0.039091	2.650869
201.406854	2261.086198	17.859251	-0.039044	2.646629
201.358504	2253.092311	17.864256	-0.039030	2.642360
201.459207	2245.133307	17.869261	-0.039044	2.638113
201.335464	2237.179160	17.874266	-0.039016	2.633848
201.235286	2229.169024	17.879271	-0.038992	2.629546
201.104510	2221.229561	17.884275	-0.038962	2.625274
201.012108	2213.254563	17.889280	-0.038940	2.620978
200.985927	2205.300402	17.894285	-0.038930	2.616690
201.140290	2197.283405	17.899290	-0.038954	2.612374
200.978252	2189.316315	17.904295	-0.038918	2.608056
201.038473	2181.365935	17.909299	-0.038924	2.603755
200.864934	2173.391097	17.914304	-0.038887	2.599418
200.779626	2165.477783	17.919309	-0.038866	2.595113
200.729822	2157.308095	17.924314	-0.038851	2.590664
200.732668	2149.332125	17.929319	-0.038847	2.586316
200.804597	2141.401450	17.934323	-0.038855	2.581991
200.594826	2133.474946	17.939328	-0.038811	2.577641
200.672008	2125.510727	17.944333	-0.038820	2.573283
200.665979	2117.536339	17.949338	-0.038814	2.568906
200.566330	2109.577149	17.954343	-0.038790	2.564523
200.485917	2101.676201	17.959347	-0.038770	2.560167
200.307476	2093.709557	17.964352	-0.038732	2.555760
200.395702	2085.714742	17.969357	-0.038743	2.551348
200.163186	2077.763742	17.974362	-0.038695	2.546930
199.952280	2069.813796	17.979367	-0.038650	2.542507
200.165286	2061.827154	17.984371	-0.038685	2.538086
199.752818	2053.897408	17.989376	-0.038603	2.533644
199.762641	2045.892581	17.994381	-0.038600	2.529182
199.618740	2037.938024	17.999386	-0.038568	2.524730
199.559902	2029.999499	18.004391	-0.038552	2.520285
199.878703	2022.007317	18.009395	-0.038606	2.515829
199.753435	2013.994800	18.014400	-0.038577	2.511322
199.709627	2006.047254	18.019405	-0.038564	2.506849
199.482071	1998.101075	18.024410	-0.038516	2.502355
199.305438	1990.156921	18.029415	-0.038478	2.497859
199.442378	1982.170338	18.034419	-0.038499	2.493353
199.200139	1974.197669	18.039424	-0.038449	2.488818
199.274298	1966.236270	18.044429	-0.038457	2.484306
199.222130	1958.285399	18.049434	-0.038442	2.479782
199.117704	1950.351484	18.054439	-0.038418	2.475255
199.044109	1942.369908	18.059443	-0.038399	2.470695
198.922880	1934.401139	18.064448	-0.038371	2.466130
198.977308	1926.444383	18.069453	-0.038376	2.461577
198.839639	1918.486956	18.074458	-0.038346	2.457001
198.681535	1910.525953	18.079463	-0.038311	2.452412
198.721454	1902.567753	18.084467	-0.038313	2.447831
198.555678	1894.605517	18.089472	-0.038277	2.443224
198.441228	1886.668632	18.094477	-0.038251	2.438627
198.487391	1878.689251	18.099482	-0.038254	2.434009
198.314687	1870.640480	18.104487	-0.038217	2.429324
198.532744	1862.666693	18.109491	-0.038252	2.424705
198.564197	1854.720891	18.114496	-0.038253	2.420078
198.317462	1846.812725	18.119501	-0.038202	2.415443
198.003538	1838.864545	18.124506	-0.038139	2.410771
197.858863	1830.891621	18.129511	-0.038107	2.406088
198.015153	1822.930337	18.134515	-0.038131	2.401426
197.873163	1814.998479	18.139520	-0.038099	2.396749
197.917653	1807.014408	18.144525	-0.038102	2.392047
197.852930	1799.054273	18.149530	-0.038085	2.387341
197.758671	1791.100645	18.154535	-0.038062	2.382627
197.724114	1783.163479	18.159539	-0.038051	2.377919
197.489521	1775.206974	18.164544	-0.038002	2.373173
197.638686	1767.219080	18.169549	-0.038025	2.368430
197.554122	1759.268901	18.174554	-0.038004	2.363681
197.598427	1751.322834	18.179559	-0.038007	2.358936
197.456330	1743.406709	18.184563	-0.037975	2.354184
197.192242	1735.407780	18.189568	-0.037921	2.349362
197.322396	1727.432431	18.194573	-0.037940	2.344577
197.447599	1719.471868	18.199578	-0.037958	2.339791
197.218199	1711.543667	18.204583	-0.037910	2.334985
197.206189	1703.575539	18.209587	-0.037903	2.330163
196.787111	1695.651602	18.214592	-0.037820	2.325325
196.886594	1687.700347	18.219597	-0.037833	2.320502
196.729894	1679.776224	18.224602	-0.037799	2.315665
196.582411	1671.789536	18.229607	-0.037766	2.310780
196.714613	1663.820512	18.234611	-0.037786	2.305918
196.706640	1655.862744	18.239616	-0.037779	2.301042
196.675731	1647.919657	18.244621	-0.037768	2.296163
196.594900	1639.969668	18.249626	-0.037748	2.291264
196.453218	1632.028673	18.254631	-0.037717	2.286356
196.345275	1624.099905	18.259635	-0.037692	2.281447
196.306329	1616.144230	18.264640	-0.037679	2.276517
196.321923	1608.140970	18.269645	-0.037677	2.271551
196.330353	1600.156429	18.274650	-0.037673	2.266586
195.986248	1592.241797	18.279655	-0.037604	2.261622
196.135281	1584.287956	18.284659	-0.037627	2.256666
196.146292	1576.314397	18.289664	-0.037624	2.251675
196.069745	1568.382874	18.294669	-0.037604	2.246691
196.008525	1560.458669	18.299674	-0.037588	2.241702
195.678577	1552.544908	18.304679	-0.037521	2.236685
195.720510	1544.595351	18.309683	-0.037524	2.231667
195.739310	1536.608260	18.314688	-0.037522	2.226612
195.729102	1528.671361	18.319693	-0.037515	2.221574
195.574785	1520.751133	18.324698	-0.037482	2.216523
195.393045	1512.799101	18.329703	-0.037443	2.211438
195.369376	1504.857356	18.334707	-0.037433	2.206361
195.377286	1496.901436	18.339712	-0.037429	2.201267
195.361694	1488.979621	18.344717	-0.037421	2.196180
195.174465	1481.031371	18.349722	-0.037381	2.191049
195.264356	1473.028752	18.354727	-0.037393	2.185896
195.068306	1465.141923	18.359731	-0.037351	2.180780
195.057219	1457.179356	18.364736	-0.037344	2.175619
195.008679	1449.236439	18.369741	-0.037330	2.170456
194.835722	1441.305017	18.374746	-0.037293	2.165276
194.755927	1433.377005	18.379751	-0.037273	2.160095
194.590199	1425.475800	18.384755	-0.037237	2.154910
194.653266	1417.483487	18.389760	-0.037243	2.149675
194.480283	1409.555765	18.394765	-0.037206	2.144447
194.389393	1401.638787	18.399770	-0.037184	2.139221
194.441282	1393.662879	18.404775	-0.037189	2.133957
194.204466	1385.761287	18.409779	-0.037139	2.128702
194.181970	1377.806236	18.414784	-0.037130	2.123419
194.352983	1369.863699	18.419789	-0.037157	2.118149
194.310462	1361.900102	18.424794	-0.037144	2.112832
194.108240	1353.935364	18.429799	-0.037101	2.107485
193.953430	1346.028745	18.434803	-0.037067	2.102167
193.937432	1338.080829	18.439808	-0.037059	2.096823
193.805891	1330.169244	18.444813	-0.037029	2.091477
193.933127	1322.196525	18.449818	-0.037048	2.086102
193.762808	1314.293513	18.454823	-0.037011	2.080731
193.764623	1306.383640	18.459827	-0.037006	2.075359
193.460440	1298.459203	18.464832	-0.036945	2.069932
193.555726	1290.498317	18.469837	-0.036957	2.064506
193.644598	1282.573321	18.474842	-0.036969	2.059089
193.233648	1274.685286	18.479847	-0.036887	2.053634
193.207209	1266.741277	18.484851	-0.036877	2.048164
193.197629	1258.801102	18.489856	-0.036870	2.042683
193.064081	1250.905178	18.494861	-0.036840	2.037206
192.920613	1242.972712	18.499866	-0.036808	2.031688
193.055670	1234.984973	18.504871	-0.036828	2.026145
193.191913	1227.051412	18.509875	-0.036849	2.020624
192.952896	1219.150295	18.514880	-0.036799	2.015072
192.923230	1211.211465	18.519885	-0.036788	2.009501
192.909226	1203.292551	18.524890	-0.036781	2.003929
192.658490	1195.412429	18.529895	-0.036729	1.998344
192.707797	1187.485470	18.534899	-0.036733	1.992742
192.527336	1179.542178	18.539904	-0.036694	1.987089
192.411616	1171.634755	18.544909	-0.036668	1.981451
192.391964	1163.720497	18.549914	-0.036659	1.975803
192.144628	1155.804469	18.554919	-0.036608	1.970113
192.361131	1147.866675	18.559923	-0.036643	1.964441
191.966784	1139.999302	18.564928	-0.036564	1.958737
192.062075	1132.044374	18.569933	-0.036577	1.953006
191.960248	1124.089948	18.574938	-0.036553	1.947237
192.007941	1116.152348	18.579943	-0.036557	1.941480
191.925857	1108.257110	18.584947	-0.036536	1.935722
192.038174	1100.302968	18.589952	-0.036552	1.929925
191.775556	1092.430652	18.594957	-0.036498	1.924129
191.670523	1084.542528	18.599962	-0.036474	1.918322
191.617841	1076.615229	18.604967	-0.036459	1.912474
191.666393	1068.694329	18.609971	-0.036463	1.906624
191.443597	1060.795509	18.614976	-0.036416	1.900741
191.407851	1052.894783	18.619981	-0.036404	1.894861
191.195182	1045.003071	18.624986	-0.036360	1.888948
191.076661	1037.095231	18.629991	-0.036332	1.883016
190.909673	1029.224954	18.634995	-0.036296	1.877087
191.011650	1021.257294	18.640000	-0.036310	1.871097
190.942318	1013.341399	18.645005	-0.036292	1.865108
190.665957	1005.476868	18.650010	-0.036236	1.859114
190.775514	997.536587	18.655015	-0.036251	1.853087
190.585403	989.652226	18.660019	-0.036210	1.847049
190.642620	981.729336	18.665024	-0.036216	1.840991
190.460606	973.863128	18.670029	-0.036177	1.834927
190.492733	965.949229	18.675034	-0.036178	1.828833
190.323557	958.056588	18.680039	-0.036141	1.822710
190.331570	950.164642	18.685043	-0.036138	1.816588
190.167078	942.269847	18.690048	-0.036102	1.810423
190.165294	934.370099	18.695053	-0.036097	1.804252
190.006445	926.509730	18.700058	-0.036062	1.798072
189.855652	918.581915	18.705063	-0.036029	1.791819
189.842644	910.659294	18.710067	-0.036021	1.785564
189.919302	902.743376	18.715072	-0.036030	1.779304
189.697248	894.887182	18.720077	-0.035984	1.773033
189.715241	886.988524	18.725082	-0.035982	1.766734
189.588883	879.107785	18.730087	-0.035954	1.760410
189.441170	871.265560	18.735091	-0.035921	1.754091
189.279894	863.368774	18.740096	-0.035886	1.747704
189.466936	855.446224	18.745101	-0.035916	1.741316
189.349388	847.597199	18.750106	-0.035889	1.734926
189.238616	839.702125	18.755111	-0.035863	1.728476
189.197266	831.838043	18.760115	-0.035850	1.722035
189.131247	823.971207	18.765120	-0.035833	1.715565
188.889170	816.098300	18.770125	-0.035783	1.709043
188.876132	808.210468	18.775130	-0.035775	1.702513
188.803625	800.344618	18.780135	-0.035757	1.695968
188.672664	792.476920	18.785139	-0.035727	1.689389
188.593095	784.592919	18.790144	-0.035707	1.682777
188.611548	776.742182	18.795149	-0.035706	1.676180
188.610345	768.856352	18.800154	-0.035700	1.669525
188.504394	760.987292	18.805159	-0.035676	1.662843
188.587061	753.124850	18.810163	-0.035686	1.656165
188.338229	745.280742	18.815168	-0.035635	1.649431
188.270002	737.423536	18.820173	-0.035617	1.642683
188.230254	729.576893	18.825178	-0.035604	1.635919
188.017518	721.670899	18.830183	-0.035560	1.629053
187.918672	713.822858	18.835187	-0.035536	1.622223
187.854184	705.963819	18.840192	-0.035519	1.615360
187.991133	698.079193	18.845197	-0.035540	1.608473
187.866877	690.249344	18.850202	-0.035511	1.601568
187.362421	682.470722	18.855207	-0.035412	1.594625
187.479545	674.595331	18.860211	-0.035429	1.587653
187.546078	666.720537	18.865216	-0.035437	1.580645
187.288908	658.923526	18.870221	-0.035384	1.573628
187.171756	651.077219	18.875226	-0.035357	1.566555
187.168201	643.238369	18.880231	-0.035351	1.559474
187.233049	635.388273	18.885235	-0.035358	1.552360
186.924034	627.553288	18.890240	-0.035296	1.545172
186.726056	619.756900	18.895245	-0.035254	1.538002
186.816221	611.889262	18.900250	-0.035265	1.530776
186.644784	604.077217	18.905255	-0.035228	1.523528
186.788636	596.245244	18.910259	-0.035250	1.516274
186.660065	588.420668	18.915264	-0.035221	1.508951
186.272403	580.648866	18.920269	-0.035144	1.501602
186.346014	572.814155	18.925274	-0.035153	1.494228
186.283599	564.980518	18.930279	-0.035136	1.486798
186.380585	557.166285	18.935283	-0.035149	1.479374
185.993936	549.378429	18.940288	-0.035072	1.471862
186.043364	541.521547	18.945293	-0.035076	1.464313
186.099684	533.716604	18.950298	-0.035082	1.456777
185.692633	525.957146	18.955303	-0.035001	1.449172
185.462417	518.187054	18.960307	-0.034953	1.441544
185.649181	510.355249	18.965312	-0.034983	1.433883
185.344779	502.590868	18.970317	-0.034921	1.426167
185.322871	494.808121	18.975322	-0.034912	1.418437
185.142959	487.018844	18.980327	-0.034873	1.410632
185.171443	479.228798	18.985331	-0.034874	1.402818
185.048363	471.467041	18.990336	-0.034846	1.394963
184.947320	463.666559	18.995341	-0.034822	1.387028
185.052345	455.876157	19.000346	-0.034836	1.379092
184.824055	448.124712	19.005351	-0.034789	1.371094
184.939291	440.339882	19.010355	-0.034805	1.363073
184.752111	432.609680	19.015360	-0.034766	1.355009
184.651709	424.854237	19.020365	-0.034742	1.346886
184.334928	417.153558	19.025370	-0.034678	1.338733
184.344414	409.368401	19.030375	-0.034675	1.330498
184.499811	401.602590	19.035379	-0.034699	1.322258
184.161430	393.886438	19.040384	-0.034631	1.313932
183.902833	386.070390	19.045389	-0.034577	1.305458
184.040734	378.321587	19.050394	-0.034598	1.297075
183.865550	370.610959	19.055399	-0.034561	1.288621
183.871384	362.896600	19.060403	-0.034557	1.280141
183.691280	355.206762	19.065408	-0.034518	1.271597
183.639768	347.491556	19.070413	-0.034504	1.262991
183.511302	339.808977	19.075418	-0.034475	1.254347
183.361239	332.110445	19.080423	-0.034442	1.245622
183.217362	324.448575	19.085427	-0.034410	1.236878
183.110537	316.739395	19.090432	-0.034385	1.228024
182.966426	309.061916	19.095437	-0.034354	1.219136
183.060958	301.361422	19.100442	-0.034366	1.210202
182.623010	293.742696	19.105447	-0.034280	1.201192
182.440864	286.112358	19.110451	-0.034241	1.192152
182.580539	278.403422	19.115456	-0.034262	1.183014
182.326094	270.789332	19.120461	-0.034210	1.173838
181.922777	263.194178	19.125466	-0.034130	1.164581
182.074748	255.512556	19.130471	-0.034153	1.155261
181.891147	247.860196	19.135475	-0.034114	1.145830
181.423329	240.302607	19.140480	-0.034022	1.136378
181.157097	232.702923	19.145485	-0.033967	1.126837
181.374373	225.049465	19.150490	-0.034003	1.117252
180.864352	217.506094	19.155495	-0.033903	1.107564
180.683968	209.937540	19.160499	-0.033865	1.097832
180.662622	202.331267	19.165504	-0.033856	1.087999
180.402505	194.792316	19.170509	-0.033803	1.078110
180.206770	187.230887	19.175514	-0.033761	1.068115
179.879317	179.704934	19.180519	-0.033695	1.058042
179.895758	172.148275	19.185523	-0.033694	1.047911
179.392984	164.678913	19.190528	-0.033595	1.037678
179.120678	157.175553	19.195533	-0.033540	1.027350
178.781015	149.709780	19.200538	-0.033472	1.016954
178.140377	142.280270	19.205543	-0.033348	1.006427
177.698374	134.850814	19.210547	-0.033260	0.995838
177.228020	127.373945	19.215552	-0.033168	0.985059
176.876593	119.934814	19.220557	-0.033098	0.974246
176.394148	112.525558	19.225562	-0.033003	0.963322
175.971285	105.125469	19.230567	-0.032920	0.952301
175.477831	97.747687	19.235571	-0.032823	0.941166
175.091840	90.363469	19.240576	-0.032747	0.929916
174.586215	83.023731	19.245581	-0.032648	0.918564
174.333687	75.647848	19.250586	-0.032596	0.907082
173.760877	68.349298	19.255591	-0.032485	0.895487
173.344990	61.272630	19.260595	-0.032403	0.884138