Thu Mar 11 20:23:04 2021

Number of Points = 3628
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.188316	-0.138516	0.000000	-0.000045	0.721154

0.164368	-0.149245	0.005005	-0.000040	0.721125
0.120344	-0.136520	0.010010	-0.000032	0.721135
0.166602	-0.150427	0.015014	-0.000041	0.721123
-0.083986	-0.103616	0.020019	0.000006	0.721128
0.011505	-0.119663	0.025024	-0.000012	0.721130
-0.050557	-0.113051	0.030029	-0.000000	0.721121
0.198628	-0.150793	0.035034	-0.000047	0.721134
0.069134	-0.133640	0.040038	-0.000023	0.721123
0.225931	-0.160128	0.045043	-0.000052	0.721126
0.335609	-0.178107	0.050048	-0.000072	0.721129
0.280251	-0.171815	0.055053	-0.000062	0.721122
0.231810	-0.157033	0.060058	-0.000053	0.721134
0.235508	-0.162488	0.065062	-0.000054	0.721125
0.365998	-0.278557	0.070067	-0.000078	0.720942
0.200855	-0.280402	0.075072	-0.000047	0.720881
0.150045	-0.275593	0.080077	-0.000038	0.720872
0.123193	-0.267118	0.085082	-0.000033	0.720880
-0.074433	-0.236125	0.090086	0.000004	0.720871
-0.025524	-0.241101	0.095091	-0.000005	0.720879
-0.018494	-0.272135	0.100096	-0.000007	0.720820
-0.007188	-0.417018	0.105101	-0.000009	0.720539
-0.043628	-0.407669	0.110106	-0.000002	0.720545
-0.082215	-0.404321	0.115110	0.000005	0.720538
0.087150	-0.431741	0.120115	-0.000026	0.720543
0.246640	-0.467116	0.125120	-0.000056	0.720530
0.149008	-0.606690	0.130125	-0.000038	0.720221
0.140603	-0.600908	0.135130	-0.000036	0.720229
-0.030943	-0.575346	0.140134	-0.000004	0.720220
0.141407	-0.604212	0.145139	-0.000037	0.720223
0.182115	-0.753935	0.150144	-0.000044	0.719943
0.048601	-0.755069	0.155149	-0.000019	0.719894
0.181071	-0.774695	0.160154	-0.000044	0.719901
0.136766	-0.800349	0.165158	-0.000036	0.719835
0.232343	-0.937952	0.170163	-0.000053	0.719598
0.043779	-0.903415	0.175168	-0.000018	0.719600
-0.053403	-0.887884	0.180173	-0.000000	0.719596
0.078887	-1.043108	0.185178	-0.000025	0.719337
-0.060964	-1.054608	0.190182	0.000001	0.719265
0.018500	-1.065550	0.195187	-0.000014	0.719272
0.003459	-1.168877	0.200192	-0.000011	0.719063
-0.087073	-1.204773	0.205197	0.000006	0.718960
-0.108317	-1.197780	0.210202	0.000010	0.718966
-0.093686	-1.326081	0.215206	0.000007	0.718718
0.042700	-1.388567	0.220211	-0.000018	0.718643
-0.013000	-1.378720	0.225216	-0.000008	0.718643
0.090337	-1.546006	0.230221	-0.000027	0.718349
0.198753	-1.560647	0.235226	-0.000047	0.718358
0.052020	-1.621219	0.240230	-0.000020	0.718187
0.137269	-1.722535	0.245235	-0.000036	0.718017
0.064624	-1.721049	0.250240	-0.000022	0.717995
-0.033132	-1.852344	0.255245	-0.000004	0.717701
-0.199886	-1.818610	0.260250	0.000027	0.717709
-0.099681	-1.955458	0.265254	0.000008	0.717474
-0.033495	-2.014771	0.270259	-0.000004	0.717380
-0.273522	-2.035439	0.275264	0.000041	0.717254
-0.465403	-2.088898	0.280269	0.000076	0.717081
-0.149380	-2.171383	0.285274	0.000018	0.717029
-0.358201	-2.275396	0.290278	0.000056	0.716750
-0.275780	-2.291177	0.295283	0.000041	0.716748
-0.347416	-2.426115	0.300288	0.000055	0.716456
-0.707054	-2.366581	0.305293	0.000121	0.716447
-1.911317	-2.290041	0.310298	0.000346	0.716174
-2.550999	-2.198665	0.315302	0.000465	0.716129
-3.100374	-2.111435	0.320307	0.000567	0.716108
-3.270787	-2.193187	0.325312	0.000599	0.715886
-3.538757	-2.149504	0.330317	0.000648	0.715878
-3.678839	-2.118401	0.335322	0.000674	0.715890
-4.219048	-2.189952	0.340326	0.000775	0.715558
-4.496339	-2.147046	0.345331	0.000827	0.715545
-4.555650	-2.134861	0.350336	0.000838	0.715548
-4.621494	-2.198665	0.355341	0.000850	0.715399
-5.631404	-2.101866	0.360346	0.001038	0.715234
-5.344854	-2.154365	0.365350	0.000984	0.715231
-5.753773	-2.082142	0.370355	0.001060	0.715230
-5.695854	-2.145416	0.375360	0.001050	0.715125
-6.412345	-2.129210	0.380365	0.001183	0.714904
-5.898863	-2.216081	0.385370	0.001087	0.714913
-6.578076	-2.099125	0.390374	0.001214	0.714905
-6.446627	-2.121712	0.395379	0.001189	0.714907
-6.667293	-2.230286	0.400384	0.001230	0.714613
-7.497915	-2.088278	0.405389	0.001385	0.714601
-7.410107	-2.099436	0.410394	0.001369	0.714610
-7.043189	-2.169281	0.415398	0.001300	0.714602
-7.516470	-2.108192	0.420403	0.001388	0.714556
-8.343245	-2.099864	0.425408	0.001542	0.714280
-8.227405	-2.123130	0.430413	0.001521	0.714275
-8.384937	-2.092152	0.435418	0.001550	0.714280
-8.543038	-2.067085	0.440422	0.001579	0.714274
-8.109384	-2.142257	0.445427	0.001499	0.714279
-8.201778	-2.212229	0.450432	0.001516	0.714107
-9.452708	-2.062142	0.455437	0.001749	0.713962
-8.920886	-2.151469	0.460442	0.001650	0.713973
-9.141280	-2.115065	0.465446	0.001691	0.713968
-9.614899	-2.031701	0.470451	0.001779	0.713966
-9.346898	-2.076616	0.475456	0.001729	0.713971
-9.384983	-2.157794	0.480461	0.001736	0.713797
-10.157430	-2.089935	0.485466	0.001880	0.713658
-10.195171	-2.086151	0.490470	0.001887	0.713652
-10.368542	-2.053805	0.495475	0.001919	0.713655
-9.946116	-2.128317	0.500480	0.001840	0.713657
-10.072710	-2.111685	0.505485	0.001864	0.713645
-10.364446	-2.085612	0.510490	0.001918	0.713594
-11.055872	-2.081298	0.515494	0.002047	0.713357
-10.901598	-2.106583	0.520499	0.002018	0.713362
-11.207771	-2.051008	0.525504	0.002075	0.713364
-11.127661	-2.070770	0.530509	0.002060	0.713353
-10.648036	-2.150334	0.535514	0.001971	0.713365
-11.257061	-2.045469	0.540518	0.002084	0.713358
-11.083808	-2.186348	0.545523	0.002052	0.713139
-11.965569	-2.083721	0.550528	0.002216	0.713030
-12.426859	-2.005644	0.555533	0.002302	0.713022
-12.297412	-2.023997	0.560538	0.002277	0.713032
-12.045359	-2.072785	0.565542	0.002231	0.713024
-12.042130	-2.071434	0.570547	0.002230	0.713028
-12.194810	-2.044814	0.575552	0.002258	0.713027
-12.403418	-2.062979	0.580557	0.002297	0.712917
-13.000986	-2.058367	0.585562	0.002408	0.712714
-12.871195	-2.084625	0.590566	0.002384	0.712708
-13.295149	-2.007356	0.595571	0.002463	0.712712
-12.861037	-2.083251	0.600576	0.002382	0.712714
-12.966017	-2.068696	0.605581	0.002402	0.712706
-13.248007	-2.014566	0.610586	0.002454	0.712714
-12.838870	-2.112786	0.615590	0.002378	0.712664
-13.614865	-2.114042	0.620595	0.002522	0.712386
-14.001293	-2.041499	0.625600	0.002594	0.712393
-14.360104	-1.982498	0.630605	0.002661	0.712384
-13.541379	-2.122616	0.635610	0.002509	0.712395
-13.818208	-2.077831	0.640614	0.002560	0.712386
-14.150153	-2.019463	0.645619	0.002622	0.712385
-13.615572	-2.120315	0.650624	0.002522	0.712374
-14.507313	-2.106877	0.655629	0.002688	0.712084
-14.937024	-2.025330	0.660634	0.002768	0.712094
-14.858433	-2.041444	0.665638	0.002754	0.712090
-14.366645	-2.130558	0.670643	0.002662	0.712087
-14.608681	-2.084175	0.675648	0.002707	0.712093
-15.030148	-2.012361	0.680653	0.002785	0.712087
-14.596672	-2.099152	0.685658	0.002705	0.712068
-15.465827	-2.100005	0.690662	0.002867	0.711758
-15.845179	-2.031112	0.695667	0.002937	0.711760
-15.568847	-2.077959	0.700672	0.002886	0.711765
-15.511203	-2.092572	0.705677	0.002875	0.711757
-15.573928	-2.075244	0.710682	0.002886	0.711769
-15.761803	-2.045755	0.715686	0.002921	0.711761
-15.697917	-2.055842	0.720691	0.002909	0.711764
-16.197345	-2.113582	0.725696	0.003002	0.711471
-16.713778	-2.032196	0.730701	0.003099	0.711450
-16.112808	-2.135564	0.735706	0.002987	0.711457
-16.308308	-2.102757	0.740710	0.003023	0.711454
-16.949914	-1.990105	0.745715	0.003142	0.711450
-16.477361	-2.070237	0.750720	0.003054	0.711458
-16.397186	-2.089763	0.755725	0.003039	0.711448
-17.011463	-2.130018	0.760730	0.003154	0.711149
-17.554693	-2.040369	0.765734	0.003255	0.711135
-17.375144	-2.071421	0.770739	0.003221	0.711137
-17.029223	-2.131143	0.775744	0.003157	0.711141
-17.747659	-2.008160	0.780749	0.003291	0.711131
-17.530121	-2.041601	0.785754	0.003250	0.711142
-17.269987	-2.091863	0.790758	0.003202	0.711134
-17.970854	-2.088701	0.795763	0.003332	0.710891
-18.073254	-2.078659	0.800768	0.003351	0.710875
-18.010484	-2.093516	0.805773	0.003339	0.710868
-18.288269	-2.039592	0.810778	0.003391	0.710876
-18.124148	-2.072196	0.815782	0.003361	0.710870
-18.166718	-2.063980	0.820787	0.003368	0.710871
-17.846929	-2.167916	0.825792	0.003309	0.710778
-19.289054	-2.035054	0.830797	0.003577	0.710530
-18.672696	-2.140081	0.835802	0.003463	0.710539
-19.022833	-2.080611	0.840806	0.003528	0.710534
-19.457909	-2.002566	0.845811	0.003609	0.710535
-19.074541	-2.068769	0.850816	0.003537	0.710539
-19.304151	-2.033201	0.855821	0.003580	0.710528
-19.126010	-2.108081	0.860826	0.003547	0.710442
-20.187080	-2.031614	0.865830	0.003744	0.710217
-20.141526	-2.039884	0.870835	0.003736	0.710217
-20.150584	-2.035570	0.875840	0.003737	0.710223
-20.480828	-1.980541	0.880845	0.003799	0.710215
-20.069257	-2.048844	0.885850	0.003722	0.710225
-20.027920	-2.059331	0.890854	0.003715	0.710219
-19.987384	-2.065652	0.895859	0.003707	0.710221
-20.102090	-2.158579	0.900864	0.003728	0.709994
-21.023213	-2.045879	0.905869	0.003900	0.709892
-20.848693	-2.070730	0.910874	0.003867	0.709904
-20.996082	-2.048402	0.915878	0.003895	0.709896
-21.184865	-2.016003	0.920883	0.003930	0.709894
-20.662558	-2.106309	0.925888	0.003832	0.709900
-21.072225	-2.037474	0.930893	0.003909	0.709891
-21.334204	-2.095980	0.935898	0.003957	0.709681
-21.780915	-2.059020	0.940902	0.004041	0.709596
-22.003002	-2.019202	0.945907	0.004082	0.709596
-21.700428	-2.071015	0.950912	0.004025	0.709601
-21.788795	-2.060218	0.955917	0.004042	0.709591
-21.713112	-2.067809	0.960922	0.004028	0.709603
-21.773592	-2.060304	0.965926	0.004039	0.709596
-21.947335	-2.155516	0.970931	0.004071	0.709344
-22.708342	-2.055538	0.975936	0.004213	0.709273
-23.043631	-1.999990	0.980941	0.004275	0.709264
-22.517531	-2.090823	0.985946	0.004177	0.709270
-22.537412	-2.090318	0.990950	0.004181	0.709264
-22.673996	-2.065620	0.995955	0.004206	0.709265
-22.729956	-2.052054	1.000960	0.004217	0.709272
-23.046237	-2.119384	1.005965	0.004276	0.709025
-23.568303	-2.059358	1.010970	0.004373	0.708959
-23.723726	-2.034149	1.015974	0.004402	0.708954
-23.514516	-2.071782	1.020979	0.004363	0.708953
-23.386422	-2.091138	1.025984	0.004339	0.708960
-23.741597	-2.031263	1.030989	0.004405	0.708953
-23.912937	-1.996355	1.035994	0.004437	0.708962
-23.790266	-2.099961	1.040998	0.004414	0.708799
-24.748382	-2.009517	1.046003	0.004592	0.708638
-24.359412	-2.075409	1.051008	0.004520	0.708645
-24.682646	-2.023719	1.056013	0.004580	0.708633
-24.526353	-2.046699	1.061018	0.004551	0.708643
-24.582214	-2.038648	1.066022	0.004561	0.708639
-24.848339	-1.990862	1.071027	0.004611	0.708640
-24.413160	-2.095541	1.076032	0.004530	0.708586
-25.378088	-2.042459	1.081037	0.004709	0.708347
-25.165996	-2.076517	1.086042	0.004670	0.708355
-25.289125	-2.057372	1.091046	0.004693	0.708349
-25.441676	-2.030100	1.096051	0.004721	0.708350
-25.575293	-2.003710	1.101056	0.004746	0.708355
-25.522518	-2.017786	1.106061	0.004736	0.708346
-25.258248	-2.089617	1.111066	0.004687	0.708296
-26.320292	-2.043388	1.116070	0.004885	0.708009
-26.375088	-2.034629	1.121075	0.004895	0.708008
-26.308886	-2.042220	1.126080	0.004882	0.708016
-26.401790	-2.028265	1.131085	0.004900	0.708011
-26.362086	-2.030549	1.136090	0.004892	0.708021
-26.421879	-2.023975	1.141094	0.004903	0.708012
-26.246242	-2.055315	1.146099	0.004871	0.708012
-26.285621	-2.177369	1.151104	0.004878	0.707754
-27.331373	-2.019807	1.156109	0.005072	0.707696
-27.168186	-2.045737	1.161114	0.005042	0.707702
-27.155112	-2.049347	1.166118	0.005040	0.707700
-27.358825	-2.013617	1.171123	0.005077	0.707699
-26.994106	-2.074651	1.176128	0.005010	0.707707
-27.144806	-2.051444	1.181133	0.005038	0.707700
-27.749341	-2.099153	1.186138	0.005150	0.707388
-28.162718	-2.031146	1.191142	0.005227	0.707376
-28.203410	-2.024122	1.196147	0.005235	0.707376
-27.697895	-2.110255	1.201152	0.005140	0.707384
-28.087876	-2.046535	1.206157	0.005213	0.707373
-27.810002	-2.092132	1.211162	0.005161	0.707380
-27.874919	-2.099848	1.216166	0.005173	0.707342
-28.857829	-2.054175	1.221171	0.005356	0.707082
-28.484251	-2.118933	1.226176	0.005287	0.707086
-28.833602	-2.060663	1.231181	0.005352	0.707078
-28.983010	-2.029555	1.236186	0.005379	0.707087
-28.674113	-2.086556	1.241190	0.005322	0.707083
-28.811200	-2.063360	1.246195	0.005347	0.707081
-28.706269	-2.143367	1.251200	0.005328	0.706958
-30.001627	-2.014448	1.256205	0.005569	0.706753
-29.440005	-2.110863	1.261210	0.005464	0.706760
-29.861305	-2.039647	1.266214	0.005543	0.706753
-29.862847	-2.039407	1.271219	0.005543	0.706753
-29.514984	-2.099117	1.276224	0.005478	0.706757
-29.650450	-2.079551	1.281229	0.005503	0.706748
-29.887338	-2.110215	1.286234	0.005547	0.706602
-30.676550	-2.047728	1.291238	0.005694	0.706445
-30.615438	-2.057996	1.296243	0.005683	0.706446
-30.627036	-2.052157	1.301248	0.005685	0.706454
-30.769870	-2.032557	1.306253	0.005712	0.706442
-30.455957	-2.085053	1.311258	0.005653	0.706449
-30.479817	-2.081534	1.316262	0.005658	0.706448
-30.831630	-2.085114	1.321267	0.005723	0.706314
-31.629117	-2.031250	1.326272	0.005871	0.706137
-31.350627	-2.084772	1.331277	0.005820	0.706129
-31.631280	-2.031710	1.336282	0.005872	0.706135
-31.536465	-2.050937	1.341286	0.005854	0.706131
-31.395851	-2.078794	1.346291	0.005828	0.706125
-31.651006	-2.028531	1.351296	0.005875	0.706135
-31.945120	-1.998537	1.356301	0.005930	0.706090
-32.248210	-2.054817	1.361306	0.005987	0.705868
-32.080068	-2.086494	1.366310	0.005955	0.705865
-32.885954	-1.942985	1.371315	0.006105	0.705865
-32.306283	-2.045539	1.376320	0.005997	0.705866
-32.319164	-2.045568	1.381325	0.006000	0.705862
-32.397670	-2.027339	1.386330	0.006014	0.705870
-32.305865	-2.071603	1.391334	0.005997	0.705814
-33.083515	-2.077220	1.396339	0.006142	0.705524
-32.801879	-2.123660	1.401344	0.006089	0.705532
-33.659359	-1.974713	1.406349	0.006249	0.705524
-33.271921	-2.039044	1.411354	0.006177	0.705534
-33.263157	-2.041533	1.416358	0.006175	0.705532
-33.842640	-1.940243	1.421363	0.006283	0.705528
-33.156500	-2.066590	1.426368	0.006155	0.705520
-33.823310	-2.102486	1.431373	0.006279	0.705208
-34.439334	-1.989948	1.436378	0.006394	0.705214
-34.402520	-1.995654	1.441382	0.006387	0.705216
-34.188301	-2.034925	1.446387	0.006347	0.705214
-34.005691	-2.064490	1.451392	0.006313	0.705220
-34.407763	-1.996879	1.456397	0.006388	0.705212
-34.257660	-2.020609	1.461402	0.006360	0.705218
-34.266297	-2.148577	1.466406	0.006362	0.704957
-35.511565	-1.960289	1.471411	0.006593	0.704889
-35.054389	-2.038185	1.476416	0.006508	0.704897
-34.804477	-2.088082	1.481421	0.006462	0.704886
-35.245438	-2.005977	1.486426	0.006544	0.704893
-35.346246	-1.988389	1.491430	0.006562	0.704892
-34.963392	-2.059390	1.496435	0.006491	0.704887
-34.998184	-2.162759	1.501440	0.006498	0.704666
-36.260992	-1.976322	1.506445	0.006733	0.704588
-36.204082	-1.982280	1.511450	0.006722	0.704597
-35.792315	-2.057933	1.516454	0.006645	0.704592
-36.259588	-1.976250	1.521459	0.006732	0.704589
-36.092293	-2.000842	1.526464	0.006701	0.704600
-35.936330	-2.033292	1.531469	0.006672	0.704590
-36.038131	-2.121257	1.536474	0.006691	0.704377
-37.018177	-2.002208	1.541478	0.006873	0.704264
-37.042495	-1.999223	1.546483	0.006878	0.704262
-36.682542	-2.060567	1.551488	0.006811	0.704268
-37.103792	-1.988945	1.556493	0.006889	0.704261
-36.721824	-2.054794	1.561498	0.006818	0.704265
-36.492974	-2.097488	1.566502	0.006775	0.704262
-37.159060	-2.090526	1.571507	0.006899	0.704036
-38.031258	-1.974767	1.576512	0.007062	0.703956
-37.612513	-2.053174	1.581517	0.006984	0.703949
-37.611293	-2.049479	1.586522	0.006983	0.703957
-37.976870	-1.986348	1.591526	0.007051	0.703953
-38.014059	-1.980217	1.596531	0.007058	0.703952
-37.446933	-2.078151	1.601536	0.006953	0.703958
-37.833135	-2.098482	1.606541	0.007025	0.703778
-38.810985	-1.993963	1.611546	0.007207	0.703637
-38.538334	-2.042492	1.616550	0.007156	0.703638
-38.815595	-1.994912	1.621555	0.007207	0.703634
-38.876793	-1.979781	1.626560	0.007219	0.703643
-38.758583	-2.005417	1.631565	0.007197	0.703633
-38.561687	-2.038545	1.636570	0.007160	0.703637
-38.780509	-2.037857	1.641574	0.007201	0.703560
-39.548656	-2.009637	1.646579	0.007344	0.703341
-38.909171	-2.119436	1.651584	0.007225	0.703349
-39.487555	-2.019828	1.656589	0.007332	0.703342
-39.370722	-2.036633	1.661594	0.007311	0.703351
-39.051159	-2.094804	1.666598	0.007251	0.703348
-39.590857	-2.002673	1.671603	0.007351	0.703340
-39.717361	-2.100723	1.676608	0.007375	0.703097
-40.326342	-2.037356	1.681613	0.007488	0.703005
-40.251494	-2.048919	1.686618	0.007474	0.703009
-40.242544	-2.052057	1.691622	0.007473	0.703006
-40.447874	-2.016680	1.696627	0.007511	0.703004
-40.091654	-2.076518	1.701632	0.007445	0.703011
-40.544557	-2.001249	1.706637	0.007529	0.703000
-41.030001	-2.038483	1.711642	0.007619	0.702750
-41.071136	-2.060386	1.716646	0.007627	0.702691
-41.358430	-2.009388	1.721651	0.007680	0.702691
-41.164434	-2.039996	1.726656	0.007644	0.702699
-41.252737	-2.030505	1.731661	0.007660	0.702686
-41.037447	-2.063325	1.736666	0.007620	0.702698
-41.185869	-2.039754	1.741670	0.007648	0.702692
-41.752690	-2.069099	1.746675	0.007753	0.702428
-42.001695	-2.050758	1.751680	0.007800	0.702376
-42.311370	-1.999475	1.756685	0.007857	0.702368
-42.114137	-2.031589	1.761690	0.007821	0.702374
-41.993234	-2.055459	1.766694	0.007798	0.702369
-42.162961	-2.024690	1.771699	0.007830	0.702371
-42.095462	-2.033363	1.776704	0.007817	0.702377
-42.392964	-2.078710	1.781709	0.007872	0.702179
-42.819305	-2.053050	1.786714	0.007952	0.702077
-42.688864	-2.075919	1.791718	0.007927	0.702078
-43.279240	-1.973424	1.796723	0.008037	0.702072
-43.083142	-2.003832	1.801728	0.008001	0.702081
-42.931352	-2.036104	1.806733	0.007972	0.702071
-42.907135	-2.039222	1.811738	0.007968	0.702073
-42.965699	-2.160962	1.816742	0.007979	0.701806
-43.675293	-2.067138	1.821747	0.008111	0.701740
-43.809491	-2.037689	1.826752	0.008136	0.701751
-43.735650	-2.055172	1.831757	0.008122	0.701743
-43.823201	-2.037898	1.836762	0.008138	0.701746
-43.974155	-2.009511	1.841766	0.008166	0.701749
-44.121321	-1.987547	1.846771	0.008194	0.701740
-43.998525	-2.147266	1.851776	0.008171	0.701462
-44.558881	-2.059909	1.856781	0.008275	0.701436
-44.960537	-1.985623	1.861786	0.008350	0.701442
-44.694440	-2.031912	1.866790	0.008300	0.701444
-44.773939	-2.022089	1.871795	0.008315	0.701435
-44.667633	-2.037302	1.876800	0.008295	0.701443
-44.923199	-1.996044	1.881805	0.008343	0.701434
-45.233460	-2.085182	1.886810	0.008401	0.701142
-45.608306	-2.026659	1.891814	0.008470	0.701125
-45.929543	-1.971992	1.896819	0.008530	0.701120
-45.374569	-2.065635	1.901824	0.008427	0.701131
-45.698604	-2.012203	1.906829	0.008487	0.701122
-45.724886	-2.006510	1.911834	0.008492	0.701124
-45.400140	-2.063568	1.916838	0.008431	0.701126
-45.464307	-2.161971	1.921843	0.008443	0.700903
-46.062470	-2.067165	1.926848	0.008555	0.700879
-46.365939	-2.015819	1.931853	0.008611	0.700874
-46.244394	-2.035255	1.936858	0.008588	0.700879
-45.991197	-2.080711	1.941862	0.008541	0.700878
-46.338632	-2.022295	1.946867	0.008606	0.700871
-46.170234	-2.160934	1.951872	0.008575	0.700651
-47.141645	-2.045228	1.956877	0.008755	0.700534
-47.301446	-2.013570	1.961882	0.008785	0.700541
-47.348747	-2.005477	1.966886	0.008794	0.700540
-47.207346	-2.033808	1.971891	0.008767	0.700534
-46.904331	-2.083259	1.976896	0.008711	0.700543
-47.327973	-2.011288	1.981901	0.008790	0.700536
-47.787660	-2.075007	1.986906	0.008875	0.700241
-47.829956	-2.074580	1.991910	0.008883	0.700226
-48.401780	-1.975025	1.996915	0.008990	0.700222
-48.003826	-2.045638	2.001920	0.008916	0.700222

-48.125631	-2.024332	2.011917	0.008938	0.700222
-48.172870	-2.016825	2.021914	0.008947	0.700220
-48.974012	-2.026502	2.031910	0.009096	0.699911
-48.946959	-2.038790	2.041907	0.009091	0.699896
-48.815421	-1.993986	2.051904	0.009066	0.700034
-48.621943	-2.014498	2.061901	0.009030	0.700063
-47.967789	-2.070236	2.071898	0.008908	0.700186
-48.253850	-2.010391	2.081894	0.008962	0.700205
-48.141136	-2.022584	2.091891	0.008940	0.700221
-48.115801	-2.027518	2.101888	0.008936	0.700220
-48.113634	-2.026780	2.111885	0.008935	0.700222
-47.945994	-2.056976	2.121882	0.008904	0.700222
-48.170594	-2.017608	2.131878	0.008946	0.700221
-48.113476	-2.028673	2.141875	0.008935	0.700219
-47.932873	-1.979480	2.151872	0.008901	0.700384
-47.168436	-2.038469	2.161869	0.008759	0.700541
-46.983138	-2.073472	2.171866	0.008724	0.700537
-47.362929	-2.008473	2.181862	0.008795	0.700532
-47.131383	-2.049719	2.191859	0.008752	0.700532
-46.619164	-2.005711	2.201856	0.008656	0.700807
-46.232670	-2.040067	2.211853	0.008584	0.700877
-46.122854	-2.060298	2.221850	0.008564	0.700876
-46.133411	-2.057250	2.231846	0.008566	0.700878
-45.985967	-2.035781	2.241843	0.008538	0.700975
-45.492675	-2.049933	2.251840	0.008446	0.701125
-45.352789	-2.074214	2.261837	0.008420	0.701126
-45.493598	-2.049637	2.271834	0.008446	0.701125
-44.949301	-2.029175	2.281830	0.008345	0.701363
-44.618137	-2.052011	2.291827	0.008283	0.701437
-44.451463	-2.080721	2.301824	0.008252	0.701439
-44.511960	-2.063633	2.311821	0.008263	0.701452
-44.001430	-2.009361	2.321818	0.008168	0.701746
-43.664998	-2.069576	2.331814	0.008105	0.701746
-43.900358	-2.027445	2.341811	0.008149	0.701746
-43.516132	-1.992854	2.351808	0.008077	0.701955
-42.718293	-2.074875	2.361805	0.007929	0.702077
-42.888665	-2.044565	2.371802	0.007960	0.702077
-43.006822	-2.003395	2.381798	0.007982	0.702118
-42.078455	-2.043736	2.391795	0.007809	0.702371
-42.049584	-2.047716	2.401792	0.007804	0.702374
-41.982718	-2.059051	2.411789	0.007791	0.702375
-41.710567	-1.994399	2.421786	0.007741	0.702604
-41.270552	-2.028064	2.431782	0.007659	0.702695
-41.475841	-1.991762	2.441779	0.007697	0.702694
-40.968098	-2.020940	2.451776	0.007602	0.702818
-40.058609	-2.087997	2.461773	0.007433	0.703010
-40.525138	-2.006587	2.471770	0.007520	0.703007
-40.150002	-2.073891	2.481766	0.007450	0.703006
-39.485863	-2.059435	2.491763	0.007326	0.703275
-39.666601	-1.994336	2.501760	0.007360	0.703341
-39.252315	-2.067961	2.511757	0.007282	0.703342
-39.516677	-1.978270	2.521754	0.007331	0.703428
-38.659765	-2.029160	2.531750	0.007172	0.703634
-38.784194	-2.007703	2.541747	0.007195	0.703632
-38.627867	-2.034870	2.551744	0.007166	0.703634
-37.727654	-2.038350	2.561741	0.006998	0.703951
-37.871391	-2.010042	2.571738	0.007025	0.703956
-37.851891	-2.014479	2.581734	0.007021	0.703955
-37.568704	-1.975671	2.591731	0.006968	0.704135
-36.999322	-2.013605	2.601728	0.006862	0.704263
-36.831254	-2.043444	2.611725	0.006831	0.704263
-36.824966	-2.024785	2.621722	0.006830	0.704303
-36.197136	-1.993272	2.631718	0.006713	0.704593
-35.793234	-2.064185	2.641715	0.006637	0.704595
-36.012647	-2.024673	2.651712	0.006678	0.704596
-35.453308	-2.036289	2.661709	0.006574	0.704774
-35.281910	-2.007630	2.671706	0.006542	0.704893
-35.070726	-2.045813	2.681702	0.006502	0.704892
-35.172449	-2.009161	2.691699	0.006521	0.704930
-34.257568	-2.030003	2.701696	0.006351	0.705216
-34.125053	-2.054162	2.711693	0.006326	0.705215
-34.347801	-2.013512	2.721690	0.006368	0.705217
-33.903235	-1.990020	2.731686	0.006285	0.705424
-33.454341	-2.019199	2.741683	0.006201	0.705527
-33.172482	-2.068466	2.751680	0.006149	0.705529
-33.275377	-2.038929	2.761677	0.006168	0.705551
-32.685256	-1.986856	2.771674	0.006058	0.705868
-32.315259	-2.053815	2.781670	0.005989	0.705866
-32.521054	-2.017898	2.791667	0.006027	0.705865
-32.053628	-2.032466	2.801664	0.005940	0.706003
-31.535594	-2.061367	2.811661	0.005843	0.706131
-31.818662	-2.011482	2.821658	0.005896	0.706130
-31.796351	-1.989521	2.831654	0.005892	0.706182
-30.924970	-2.013725	2.841651	0.005729	0.706446
-30.527829	-2.082799	2.851648	0.005655	0.706449
-30.879909	-2.019057	2.861645	0.005721	0.706451
-30.112622	-2.052819	2.871642	0.005578	0.706658
-29.939248	-2.034730	2.881638	0.005546	0.706757
-29.960644	-2.032425	2.891635	0.005549	0.706754
-29.665057	-2.059852	2.901632	0.005494	0.706805
-29.258585	-1.991093	2.911629	0.005419	0.707089
-29.205406	-2.000096	2.921626	0.005409	0.707090
-29.148496	-2.012918	2.931622	0.005398	0.707085
-28.570131	-1.988485	2.941619	0.005290	0.707341
-28.421429	-1.994536	2.951616	0.005262	0.707382
-28.351588	-2.006119	2.961613	0.005249	0.707384
-27.816417	-2.005057	2.971610	0.005150	0.707577
-27.433611	-2.010476	2.981606	0.005078	0.707703
-27.497966	-1.998373	2.991603	0.005090	0.707705
-27.317545	-2.003091	3.001600	0.005057	0.707760
-26.655576	-1.991946	3.011597	0.004933	0.708019
-26.512452	-2.018656	3.021594	0.004906	0.708017
-26.529884	-2.016787	3.031590	0.004910	0.708015
-25.987351	-1.983368	3.041587	0.004809	0.708275
-25.494140	-2.030511	3.051584	0.004717	0.708357
-25.690653	-1.996335	3.061581	0.004753	0.708356
-25.420431	-2.021516	3.071578	0.004703	0.708402
-24.974365	-1.980893	3.081574	0.004620	0.708643
-24.805649	-2.012944	3.091571	0.004588	0.708639
-24.547600	-2.058264	3.101568	0.004540	0.708640
-24.402497	-1.975979	3.111565	0.004513	0.708857
-23.960992	-2.003523	3.121562	0.004431	0.708960
-23.996599	-1.998339	3.131558	0.004437	0.708957
-23.767163	-1.992921	3.141555	0.004394	0.709050
-23.015579	-2.019908	3.151552	0.004254	0.709264
-22.987646	-2.021402	3.161549	0.004249	0.709272
-23.035127	-2.014024	3.171546	0.004258	0.709270
-22.404024	-1.985512	3.181542	0.004140	0.709552
-22.046498	-2.024175	3.191539	0.004074	0.709602
-22.064467	-2.021746	3.201536	0.004077	0.709601
-22.083215	-1.980492	3.211533	0.004080	0.709677
-21.294484	-2.009499	3.221530	0.003933	0.709900
-21.449493	-1.983273	3.231526	0.003962	0.709897
-21.438615	-1.986297	3.241523	0.003960	0.709895
-20.841031	-1.936777	3.251520	0.003849	0.710207
-20.347047	-2.017331	3.261517	0.003757	0.710222
-20.265473	-2.031976	3.271514	0.003741	0.710222
-20.308199	-1.943269	3.281510	0.003749	0.710384
-19.521356	-2.007894	3.291507	0.003603	0.710535
-19.640432	-1.984200	3.301504	0.003625	0.710540
-19.502955	-2.002039	3.311501	0.003599	0.710554
-18.602256	-2.001249	3.321498	0.003431	0.710876
-18.661129	-1.990005	3.331494	0.003442	0.710878
-18.566264	-2.006627	3.341491	0.003425	0.710878
-18.636514	-1.940424	3.351488	0.003438	0.710986
-17.696660	-2.027621	3.361485	0.003263	0.711146
-17.894813	-1.993281	3.371482	0.003299	0.711144
-17.838852	-2.002930	3.381478	0.003289	0.711145
-16.860907	-2.019480	3.391475	0.003107	0.711460
-17.034855	-1.988044	3.401472	0.003139	0.711461
-16.729182	-2.040858	3.411469	0.003082	0.711464
-16.717629	-1.972413	3.421466	0.003080	0.711605
-15.969751	-2.024968	3.431462	0.002940	0.711766
-16.089223	-2.004337	3.441459	0.002963	0.711765
-16.033163	-2.012318	3.451456	0.002952	0.711769
-15.165479	-2.016283	3.461453	0.002790	0.712069
-15.291608	-1.979015	3.471450	0.002814	0.712099
-14.915384	-2.046514	3.481446	0.002744	0.712098
-15.081351	-1.969044	3.491443	0.002775	0.712194
-14.323635	-2.004091	3.501440	0.002633	0.712393
-14.197116	-2.027606	3.511437	0.002610	0.712391
-14.359073	-1.996385	3.521434	0.002640	0.712396
-13.560115	-1.995025	3.531430	0.002491	0.712683
-13.225382	-2.037779	3.541427	0.002429	0.712716
-13.226370	-2.037437	3.551424	0.002429	0.712717
-13.367932	-1.965842	3.561421	0.002455	0.712809
-12.554817	-1.999000	3.571418	0.002304	0.713032
-12.301404	-2.045871	3.581414	0.002256	0.713028
-12.335657	-2.039680	3.591411	0.002263	0.713029
-11.793640	-2.023161	3.601408	0.002162	0.713254
-11.212973	-2.067952	3.611405	0.002053	0.713371
-11.261131	-2.061130	3.621402	0.002062	0.713367
-11.101699	-2.088898	3.631398	0.002033	0.713369
-10.635837	-2.075927	3.641395	0.001946	0.713560
-10.159395	-2.109510	3.651392	0.001857	0.713662
-10.253713	-2.091831	3.661389	0.001875	0.713664
-10.196917	-2.102688	3.671386	0.001864	0.713663
-9.771434	-2.084602	3.681382	0.001785	0.713849
-9.477565	-2.073089	3.691379	0.001730	0.713976
-9.516578	-2.066719	3.701376	0.001737	0.713975
-9.101817	-2.138952	3.711373	0.001660	0.713979
-8.882388	-2.066801	3.721370	0.001619	0.714200
-8.316481	-2.125399	3.731366	0.001513	0.714284
-8.514333	-2.091557	3.741363	0.001550	0.714281
-8.265284	-2.135092	3.751360	0.001504	0.714283
-7.905521	-2.035424	3.761357	0.001437	0.714608
-7.493586	-2.105536	3.771354	0.001360	0.714615
-7.472089	-2.110852	3.781350	0.001356	0.714612
-7.602044	-2.023640	3.791347	0.001380	0.714740
-6.522601	-2.128363	3.801344	0.001179	0.714914
-6.538027	-2.124187	3.811341	0.001182	0.714917
-6.761730	-2.085270	3.821338	0.001223	0.714915
-5.922378	-2.101380	3.831334	0.001067	0.715180
-6.118555	-2.039199	3.841331	0.001103	0.715234
-5.755362	-2.102748	3.851328	0.001036	0.715236
-5.662678	-2.078547	3.861325	0.001018	0.715317
-4.791793	-2.115605	3.871322	0.000856	0.715551
-4.943605	-2.088670	3.881318	0.000884	0.715551
-5.064604	-2.068800	3.891315	0.000907	0.715548
-4.004085	-2.138256	3.901312	0.000709	0.715785
-4.068717	-2.072707	3.911309	0.000721	0.715892
-3.745127	-2.130420	3.921306	0.000661	0.715892
-3.763918	-2.128010	3.931302	0.000664	0.715891
-3.416222	-2.092197	3.941299	0.000599	0.716084
-3.050783	-2.128526	3.951296	0.000531	0.716142
-3.218566	-2.097957	3.961293	0.000562	0.716143
-2.901769	-2.105377	3.971290	0.000503	0.716240
-2.484344	-2.071870	3.981286	0.000426	0.716454
-2.325546	-2.099160	3.991283	0.000396	0.716456
-2.290418	-2.105132	4.001280	0.000389	0.716457
-1.779212	-2.040635	4.011277	0.000294	0.716765
-1.717316	-2.053112	4.021274	0.000282	0.716762
-1.684378	-2.059285	4.031270	0.000276	0.716762
-1.604972	-1.928786	4.041267	0.000261	0.717048
-1.589864	-1.909859	4.051264	0.000258	0.717091
-1.399841	-1.898459	4.061261	0.000223	0.717181
-1.197043	-1.831196	4.071258	0.000185	0.717385
-1.100834	-1.850180	4.081254	0.000167	0.717382
-1.035075	-1.711786	4.091251	0.000155	0.717678
-1.081276	-1.688482	4.101248	0.000163	0.717708
-0.815417	-1.604527	4.111245	0.000114	0.717968
-0.729256	-1.592490	4.121242	0.000097	0.718022
-0.712851	-1.455379	4.131238	0.000094	0.718299
-0.676691	-1.426825	4.141235	0.000087	0.718368
-0.845522	-1.254161	4.151232	0.000119	0.718650
-0.611987	-1.226252	4.161229	0.000075	0.718787
-0.714425	-1.116233	4.171226	0.000094	0.718968
-0.602598	-0.993197	4.181222	0.000073	0.719251
-0.627271	-0.890666	4.191219	0.000077	0.719444
-0.455595	-0.817843	4.201216	0.000045	0.719648
-0.435326	-0.691216	4.211213	0.000041	0.719905
-0.464189	-0.546944	4.221210	0.000047	0.720179
-0.269686	-0.459186	4.231206	0.000010	0.720420
-0.184733	-0.345644	4.241203	-0.000006	0.720674
-0.103605	-0.227483	4.251200	-0.000021	0.720935
-0.079526	-0.121086	4.261197	-0.000026	0.721153
-0.047409	0.021949	4.271194	-0.000032	0.721445
0.000000	0.200064	4.281190	-0.000041	0.721812

-0.052691	0.813244	4.286195	-0.000031	0.722998
0.141748	2.038249	4.291200	-0.000068	0.725465
0.445484	3.841011	4.296205	-0.000126	0.729087
0.789572	6.193205	4.301210	-0.000192	0.733767
0.953724	9.077417	4.306214	-0.000224	0.739378
1.349333	12.409481	4.311219	-0.000300	0.745876
1.610985	16.214462	4.316224	-0.000351	0.753165
1.760953	20.443633	4.321229	-0.000382	0.761138
2.190768	25.023643	4.326234	-0.000465	0.769766
2.577495	29.969947	4.331238	-0.000540	0.778952
3.250773	35.226714	4.336243	-0.000669	0.788681
3.704056	40.835804	4.341248	-0.000757	0.798847
4.161560	46.748974	4.346253	-0.000846	0.809420
4.678536	52.942216	4.351258	-0.000947	0.820358
5.331334	59.370279	4.356262	-0.001073	0.831594
7.027441	65.861429	4.361267	-0.001393	0.843096
8.015415	72.710306	4.366272	-0.001581	0.854828
8.767550	79.813024	4.371277	-0.001726	0.866748
9.395541	87.128443	4.376282	-0.001848	0.878815
9.959171	94.621868	4.381286	-0.001957	0.890982
10.512218	102.280629	4.386291	-0.002065	0.903243
11.363613	110.027194	4.391296	-0.002229	0.915555
12.328852	117.872041	4.396301	-0.002414	0.927885
13.253428	125.863627	4.401306	-0.002591	0.940263
13.644718	134.037445	4.406310	-0.002669	0.952611
14.531094	142.221919	4.411315	-0.002840	0.964945
15.335699	150.502422	4.416320	-0.002995	0.977241
15.926752	158.904481	4.421325	-0.003111	0.989504
16.750818	167.321043	4.426330	-0.003270	1.001695
17.399151	175.795009	4.431334	-0.003396	1.013776
17.974676	184.330569	4.436339	-0.003509	1.025782
18.879063	192.834838	4.441344	-0.003683	1.037684
19.918490	201.339190	4.446349	-0.003882	1.049483
20.619863	209.941860	4.451354	-0.004018	1.061203
20.968339	218.628428	4.456358	-0.004089	1.072824
21.813613	227.225146	4.461363	-0.004252	1.084316
22.605325	235.846368	4.466368	-0.004405	1.095706
23.462909	244.460291	4.471373	-0.004570	1.106984
24.268468	253.102573	4.476378	-0.004726	1.118172
24.807392	261.765997	4.481382	-0.004832	1.129218
25.583384	270.408040	4.486387	-0.004982	1.140181
25.886399	279.131903	4.491392	-0.005044	1.151040
26.658772	287.746099	4.496397	-0.005194	1.161761
27.675178	296.306241	4.501402	-0.005388	1.172369
28.085451	304.954718	4.506406	-0.005470	1.182863
28.614398	313.590677	4.511411	-0.005575	1.193274
29.224872	322.171026	4.516416	-0.005694	1.203546
29.904807	330.753381	4.521421	-0.005826	1.213746
30.542182	339.324873	4.526426	-0.005950	1.223840
31.139093	347.900107	4.531430	-0.006067	1.233847
31.895083	356.416650	4.536435	-0.006214	1.243738
32.519649	364.948211	4.541440	-0.006335	1.253542
33.068250	373.471160	4.546445	-0.006443	1.263245
33.752789	381.980716	4.551450	-0.006576	1.272885
34.160639	390.495482	4.556454	-0.006658	1.282407
34.548602	399.008873	4.561459	-0.006736	1.291852
35.016055	407.492267	4.566464	-0.006828	1.301211
35.690284	415.993644	4.571469	-0.006959	1.310560
36.048571	424.533350	4.576474	-0.007032	1.319827
36.494879	432.946399	4.581478	-0.007120	1.328909
37.276882	441.324999	4.586483	-0.007271	1.337953
37.789673	449.716265	4.591488	-0.007372	1.346901
38.098501	458.157599	4.596493	-0.007435	1.355807
38.880503	466.481172	4.601498	-0.007586	1.364615
39.384491	474.859498	4.606502	-0.007686	1.373374
39.753594	483.261628	4.611507	-0.007760	1.382079
40.374149	491.609609	4.616512	-0.007881	1.390716
41.125003	499.937563	4.621517	-0.008026	1.399302
41.775817	508.263860	4.626522	-0.008153	1.407817
42.171662	516.629953	4.631526	-0.008232	1.416277
42.953483	524.923787	4.636531	-0.008383	1.424679
42.978864	533.350462	4.641536	-0.008393	1.433040
43.529748	541.645857	4.646541	-0.008501	1.441308
43.968507	549.972100	4.651546	-0.008589	1.449540
44.395818	558.282402	4.656550	-0.008674	1.457709
44.787724	566.589918	4.661555	-0.008752	1.465823
45.077381	574.960364	4.666560	-0.008811	1.473937
45.666543	583.201797	4.671565	-0.008927	1.481930
46.200811	591.462754	4.676570	-0.009032	1.489890
46.305383	599.787396	4.681574	-0.009056	1.497802
46.905498	608.015327	4.686579	-0.009174	1.505657
47.437884	616.278591	4.691584	-0.009278	1.513493
47.863367	624.529919	4.696589	-0.009363	1.521262
48.476594	632.765194	4.701594	-0.009482	1.529004
48.773220	641.048576	4.706598	-0.009543	1.536704
49.339980	649.276005	4.711603	-0.009654	1.544355
49.471202	657.595889	4.716608	-0.009684	1.551987
49.920327	665.817872	4.721613	-0.009773	1.559540
50.381594	674.030003	4.726618	-0.009864	1.567049
50.668783	682.283862	4.731622	-0.009923	1.574535
51.210944	690.479987	4.736627	-0.010029	1.581970
51.890294	698.662448	4.741632	-0.010161	1.589377
52.301321	706.898225	4.746637	-0.010243	1.596759
52.532048	715.146984	4.751642	-0.010292	1.604093
53.102897	723.335213	4.756646	-0.010403	1.611388
53.495635	731.570882	4.761651	-0.010482	1.618667
53.977540	739.757461	4.766656	-0.010577	1.625882
54.575384	747.995226	4.771661	-0.010694	1.633126
54.985522	756.201365	4.776666	-0.010775	1.640284
55.237064	764.408139	4.781670	-0.010828	1.647390
55.910861	772.578882	4.786675	-0.010958	1.654492
56.152674	780.782613	4.791680	-0.011009	1.661533
56.559699	788.973515	4.796685	-0.011090	1.668556
56.925922	797.188154	4.801690	-0.011163	1.675564
57.114353	805.376037	4.806694	-0.011204	1.682496
57.559026	813.544914	4.811699	-0.011292	1.689417
57.956193	821.729513	4.816704	-0.011371	1.696318
58.461297	829.878675	4.821709	-0.011471	1.703174
59.070429	838.037874	4.826714	-0.011590	1.710025
59.261580	846.245557	4.831718	-0.011631	1.716834
59.912671	854.383348	4.836723	-0.011757	1.723618
60.362569	862.540681	4.841728	-0.011846	1.730366
60.449708	870.765610	4.846733	-0.011868	1.737096
60.634726	878.961871	4.851738	-0.011908	1.743789
61.177473	887.086034	4.856742	-0.012014	1.750443
61.594168	895.260029	4.861747	-0.012097	1.757096
61.807191	903.428613	4.866752	-0.012142	1.763694
62.062418	911.591014	4.871757	-0.012195	1.770268
62.733798	919.721816	4.876762	-0.012325	1.776843
62.997967	927.878122	4.881766	-0.012380	1.783365
63.230274	936.076822	4.886771	-0.012428	1.789892
63.739315	944.234088	4.891776	-0.012529	1.796396
63.993775	952.383557	4.896781	-0.012581	1.802840
64.348570	960.506255	4.901786	-0.012653	1.809251
64.690923	968.647048	4.906790	-0.012722	1.815653
65.157324	976.767464	4.911795	-0.012814	1.822031
65.350345	984.931106	4.916800	-0.012855	1.828388
65.697594	993.084269	4.921805	-0.012925	1.834733
66.322606	1001.172992	4.926810	-0.013047	1.841038
66.530799	1009.322663	4.931814	-0.013091	1.847320
66.930157	1017.488367	4.936819	-0.013171	1.853616
67.508189	1025.582908	4.941824	-0.013284	1.859856
67.755149	1033.734205	4.946829	-0.013335	1.866080
68.310470	1041.885705	4.951834	-0.013444	1.872319
68.445867	1050.044254	4.956838	-0.013474	1.878494
68.875397	1058.145113	4.961843	-0.013560	1.884639
69.125272	1066.281386	4.966848	-0.013612	1.890771
69.628306	1074.388509	4.971853	-0.013711	1.896889
69.979154	1082.518089	4.976858	-0.013781	1.902987
70.171363	1090.657283	4.981862	-0.013822	1.909054
70.700066	1098.769755	4.986867	-0.013926	1.915120
70.974011	1106.887412	4.991872	-0.013982	1.921143
71.522827	1114.957028	4.996877	-0.014090	1.927141
72.050584	1123.100010	5.001882	-0.014194	1.933173
72.325753	1131.227170	5.006886	-0.014250	1.939146
72.602688	1139.351504	5.011891	-0.014307	1.945098
72.955761	1147.511287	5.016896	-0.014378	1.951067
73.304951	1155.643018	5.021901	-0.014448	1.956996
73.799452	1163.725383	5.026906	-0.014546	1.962888
73.993667	1171.834389	5.031910	-0.014587	1.968749
74.197552	1179.979800	5.036915	-0.014631	1.974619
74.688322	1188.054014	5.041920	-0.014727	1.980451
74.868154	1196.166794	5.046925	-0.014766	1.986261
75.238518	1204.281749	5.051930	-0.014840	1.992076
75.633938	1212.378909	5.056934	-0.014919	1.997863
76.135214	1220.449285	5.061939	-0.015018	2.003626
76.390102	1228.566313	5.066944	-0.015071	2.009379
76.684001	1236.690175	5.071949	-0.015131	2.015124
77.110792	1244.780411	5.076954	-0.015216	2.020844
77.466300	1252.873389	5.081958	-0.015287	2.026541
77.755392	1261.030839	5.086963	-0.015346	2.032261
78.062440	1269.123931	5.091968	-0.015409	2.037922
78.164790	1277.238549	5.096973	-0.015433	2.043561
78.493206	1285.350866	5.101978	-0.015500	2.049206
78.928999	1293.421600	5.106982	-0.015586	2.054817
79.266033	1301.511949	5.111987	-0.015654	2.060416
79.731927	1309.586617	5.116992	-0.015746	2.066003
79.977387	1317.721189	5.121997	-0.015797	2.071593
80.305108	1325.834113	5.127002	-0.015864	2.077161
80.687696	1333.884607	5.132006	-0.015940	2.082678
80.960775	1341.993411	5.137011	-0.015996	2.088208
81.071505	1350.131352	5.142016	-0.016022	2.093728
81.395519	1358.206929	5.147021	-0.016088	2.099211
81.688278	1366.300987	5.152026	-0.016148	2.104690
81.773761	1374.430994	5.157030	-0.016169	2.110159
82.362883	1382.541877	5.162035	-0.016284	2.115649
82.698853	1390.586353	5.167040	-0.016352	2.121056
82.736937	1398.686554	5.172045	-0.016364	2.126458
83.232383	1406.759021	5.177050	-0.016462	2.131871
83.607510	1414.821355	5.182054	-0.016537	2.137253
83.870992	1422.915596	5.187059	-0.016591	2.142631
84.180946	1431.001463	5.192064	-0.016654	2.147995
84.720920	1439.061826	5.197069	-0.016760	2.153350
85.312620	1447.124572	5.202074	-0.016876	2.158698
85.291555	1455.243142	5.207078	-0.016877	2.164012
85.823498	1463.305765	5.212083	-0.016981	2.169327
86.134318	1471.415474	5.217088	-0.017045	2.174640
86.174864	1479.523300	5.222093	-0.017057	2.179914
86.673832	1487.592524	5.227098	-0.017156	2.185192
86.905544	1495.699446	5.232102	-0.017204	2.190457
87.357231	1503.792761	5.237107	-0.017293	2.195721
87.303071	1511.894758	5.242112	-0.017289	2.200931
87.705232	1519.931357	5.247117	-0.017369	2.206129
88.081572	1528.023295	5.252122	-0.017444	2.211348
88.280796	1536.108207	5.257126	-0.017487	2.216533
88.654415	1544.172761	5.262131	-0.017561	2.221709
89.111339	1552.216469	5.267136	-0.017652	2.226867
89.111520	1560.346604	5.272141	-0.017657	2.232028
89.463206	1568.427637	5.277146	-0.017728	2.237176
89.772111	1576.478368	5.282150	-0.017791	2.242290
89.896331	1584.581408	5.287155	-0.017819	2.247409
90.217042	1592.666705	5.292160	-0.017884	2.252522
90.713777	1600.711510	5.297165	-0.017982	2.257613
91.023673	1608.786067	5.302170	-0.018045	2.262695
91.047561	1616.896420	5.307174	-0.018055	2.267764
91.358029	1625.033892	5.312179	-0.018118	2.272862
91.839019	1633.069278	5.317184	-0.018213	2.277900
91.917948	1641.125955	5.322189	-0.018233	2.282906
92.303464	1649.189645	5.327194	-0.018310	2.287931
92.418165	1657.280316	5.332198	-0.018337	2.292939
93.001129	1665.316500	5.337203	-0.018450	2.297942
93.335675	1673.369418	5.342208	-0.018518	2.302924
93.576723	1681.445455	5.347213	-0.018568	2.307900
93.935525	1689.531141	5.352218	-0.018640	2.312882
94.037319	1697.594997	5.357222	-0.018664	2.317818
94.178761	1705.682243	5.362227	-0.018696	2.322762
94.565694	1713.715340	5.367232	-0.018773	2.327682
94.821745	1721.799489	5.372237	-0.018826	2.332612
95.203643	1729.862149	5.377242	-0.018903	2.337528
95.265418	1737.933834	5.382246	-0.018920	2.342414
95.537823	1746.016139	5.387251	-0.018976	2.347313
95.830401	1754.118762	5.392256	-0.019035	2.352215
96.104255	1762.168991	5.397261	-0.019092	2.357074
96.508086	1770.211444	5.402266	-0.019172	2.361929
96.703934	1778.254109	5.407270	-0.019214	2.366758
96.891519	1786.363386	5.412275	-0.019254	2.371615
97.262706	1794.413616	5.417280	-0.019329	2.376442
97.429036	1802.474861	5.422285	-0.019365	2.381250
97.702482	1810.559225	5.427290	-0.019421	2.386070
98.204642	1818.579133	5.432294	-0.019520	2.390860
98.563265	1826.669277	5.437299	-0.019592	2.395670
98.782791	1834.724564	5.442304	-0.019638	2.400440
98.901815	1842.781551	5.447309	-0.019665	2.405193
99.296908	1850.844959	5.452314	-0.019744	2.409961
99.566447	1858.930098	5.457318	-0.019800	2.414724
99.750117	1867.009136	5.462323	-0.019839	2.419466
100.252603	1875.037051	5.467328	-0.019938	2.424194
100.336757	1883.131480	5.472333	-0.019959	2.428920
100.747931	1891.256021	5.477338	-0.020041	2.433678
100.955290	1899.280739	5.482342	-0.020085	2.438354
101.210215	1907.331187	5.487347	-0.020138	2.443040
101.448724	1915.374572	5.492352	-0.020187	2.447711
101.624324	1923.431460	5.497357	-0.020225	2.452376
102.067547	1931.478763	5.502362	-0.020313	2.457046
102.267676	1939.518345	5.507366	-0.020356	2.461686
102.527020	1947.589716	5.512371	-0.020409	2.466339
102.822116	1955.667477	5.517376	-0.020470	2.470989
103.009515	1963.727150	5.522381	-0.020510	2.475613
103.337203	1971.781850	5.527386	-0.020576	2.480235
103.495601	1979.832105	5.532390	-0.020611	2.484833
103.741351	1987.904460	5.537395	-0.020662	2.489442
103.921092	1995.981222	5.542400	-0.020701	2.494041
104.185303	2004.003906	5.547405	-0.020755	2.498606
104.558637	2012.065746	5.552410	-0.020830	2.503192
104.783875	2020.113556	5.557414	-0.020877	2.507752
104.946749	2028.230220	5.562419	-0.020913	2.512338
105.259394	2036.278962	5.567424	-0.020976	2.516888
105.599531	2044.298873	5.572429	-0.021045	2.521415
105.917165	2052.359442	5.577434	-0.021109	2.525955
106.217541	2060.388055	5.582438	-0.021170	2.530468
106.575859	2068.464083	5.587443	-0.021242	2.535004
106.675521	2076.506520	5.592448	-0.021266	2.539494
106.953717	2084.543610	5.597453	-0.021323	2.543986
107.445841	2092.616541	5.602458	-0.021420	2.548505
107.941111	2100.651587	5.607462	-0.021518	2.552995
108.269080	2108.704520	5.612467	-0.021584	2.557475
108.477052	2116.756435	5.617472	-0.021628	2.561939
108.721968	2124.799731	5.622477	-0.021679	2.566392
108.922173	2132.899971	5.627482	-0.021722	2.570866
109.177694	2140.970815	5.632486	-0.021775	2.575320
109.481351	2149.003325	5.637491	-0.021836	2.579748
109.799765	2157.041416	5.642496	-0.021901	2.584172
109.787516	2165.133814	5.647501	-0.021904	2.588596
110.204618	2173.325399	5.652506	-0.021987	2.593096
110.539155	2181.352852	5.657510	-0.022055	2.597493
110.901192	2189.324343	5.662515	-0.022127	2.601854
111.238147	2197.341902	5.667520	-0.022195	2.606231
111.519243	2205.368286	5.672525	-0.022253	2.610602
111.747544	2213.465373	5.677530	-0.022301	2.615000
111.800356	2221.491023	5.682534	-0.022316	2.619340
112.094663	2229.532263	5.687539	-0.022376	2.623697
112.461004	2237.561611	5.692544	-0.022449	2.628045
112.482616	2245.646756	5.697549	-0.022459	2.632394
112.672349	2253.700119	5.702554	-0.022499	2.636729
112.817086	2261.727205	5.707558	-0.022531	2.641040
113.095117	2269.759007	5.712563	-0.022588	2.645355
113.278139	2277.809902	5.717568	-0.022628	2.649667
113.575076	2285.874140	5.722573	-0.022688	2.653987
113.859581	2293.905093	5.727578	-0.022747	2.658281
114.108170	2301.939485	5.732582	-0.022798	2.662567
114.466411	2309.992454	5.737587	-0.022870	2.666864
114.757338	2318.075079	5.742592	-0.022930	2.671165
114.974596	2326.138511	5.747597	-0.022975	2.675444
115.097934	2334.186741	5.752602	-0.023004	2.679702
115.270098	2342.203420	5.757606	-0.023041	2.683940
115.709253	2350.230269	5.762611	-0.023128	2.688193
115.922853	2358.302082	5.767616	-0.023173	2.692449
116.125530	2366.362513	5.772621	-0.023216	2.696692
116.529309	2374.395462	5.777626	-0.023297	2.700926
116.563124	2382.425976	5.782630	-0.023308	2.705128
116.608619	2390.498715	5.787635	-0.023322	2.709348
116.952609	2398.574090	5.792640	-0.023391	2.713580
117.026615	2406.607544	5.797645	-0.023410	2.717767
117.737834	2414.624860	5.802650	-0.023548	2.721979
117.700190	2422.663588	5.807654	-0.023546	2.726149
117.945998	2430.732738	5.812659	-0.023597	2.730346
118.066265	2438.808834	5.817664	-0.023625	2.734532
118.381423	2446.809564	5.822669	-0.023689	2.738685
118.636641	2454.854555	5.827674	-0.023742	2.742851
118.805347	2462.890006	5.832678	-0.023778	2.747000
119.312280	2470.938503	5.837683	-0.023878	2.751170
119.711312	2479.062722	5.842688	-0.023958	2.755366
119.676628	2487.079337	5.847693	-0.023957	2.759474
119.902595	2495.113289	5.852698	-0.024004	2.763601
120.075320	2503.108175	5.857702	-0.024041	2.767698
120.356819	2511.167166	5.862707	-0.024099	2.771829
120.548087	2519.234787	5.867712	-0.024140	2.775952
120.984691	2527.226970	5.872717	-0.024226	2.780045
121.331071	2535.263209	5.877722	-0.024296	2.784149
121.462469	2543.318026	5.882726	-0.024326	2.788244
121.402495	2551.423007	5.887731	-0.024320	2.792347
121.671837	2559.470855	5.892736	-0.024376	2.796435
121.939070	2567.462849	5.897741	-0.024431	2.800488
122.332325	2575.467510	5.902746	-0.024509	2.804548
122.581051	2583.522369	5.907750	-0.024561	2.808620
122.670021	2591.621734	5.912755	-0.024583	2.812699
122.989594	2599.648570	5.917760	-0.024647	2.816749
123.237245	2607.654900	5.922765	-0.024699	2.820778
123.522805	2615.710282	5.927770	-0.024757	2.824829
123.697564	2623.778809	5.932774	-0.024795	2.828874
123.891008	2631.838715	5.937779	-0.024836	2.832910
124.152597	2639.874899	5.942784	-0.024890	2.836932
124.291142	2647.900867	5.947789	-0.024921	2.840936
124.477868	2655.918950	5.952794	-0.024961	2.844933
124.983808	2663.921688	5.957798	-0.025061	2.848935
125.428058	2671.975078	5.962803	-0.025149	2.852953
125.336346	2680.060844	5.967808	-0.025137	2.856952
125.411459	2688.111287	5.972813	-0.025156	2.860936
125.669109	2696.123986	5.977818	-0.025210	2.864907
125.716515	2704.178539	5.982822	-0.025224	2.868881
125.882812	2712.239843	5.987827	-0.025260	2.872859
126.491670	2720.254616	5.992832	-0.025379	2.876834
126.559850	2728.279516	5.997837	-0.025396	2.880778
126.962104	2736.295392	6.002842	-0.025477	2.884730
127.271418	2744.330286	6.007846	-0.025540	2.888681
127.505386	2752.394956	6.012851	-0.025588	2.892638
127.439909	2760.485478	6.017856	-0.025581	2.896585
127.878669	2768.475412	6.022861	-0.025668	2.900505
127.976933	2776.524317	6.027866	-0.025692	2.904430
128.104435	2784.588009	6.032870	-0.025721	2.908358
128.292556	2792.671440	6.037875	-0.025761	2.912294
128.637970	2800.744104	6.042880	-0.025831	2.916228
129.028694	2808.700980	6.047885	-0.025909	2.920102
129.239494	2816.723239	6.052890	-0.025953	2.923994
129.220585	2824.772385	6.057894	-0.025955	2.927881
129.534948	2832.794531	6.062899	-0.026019	2.931768
129.649696	2840.882980	6.067904	-0.026046	2.935671
129.570544	2848.876098	6.072909	-0.026036	2.939512
129.988088	2856.924504	6.077914	-0.026119	2.943401
130.106197	2864.947247	6.082918	-0.026147	2.947257
130.406808	2872.987539	6.087923	-0.026208	2.951126
130.814366	2881.033522	6.092928	-0.026289	2.954998
130.985026	2889.030864	6.097933	-0.026326	2.958829
131.192105	2897.087105	6.102938	-0.026370	2.962686
131.618038	2905.089155	6.107942	-0.026454	2.966522
131.894157	2913.132305	6.112947	-0.026511	2.970366
132.078500	2921.220819	6.117952	-0.026551	2.974221
132.063849	2929.251074	6.122957	-0.026553	2.978034
132.377319	2937.277693	6.127962	-0.026617	2.981856
132.507574	2945.314507	6.132966	-0.026646	2.985669
132.828880	2953.340044	6.137971	-0.026711	2.989482
133.159669	2961.437154	6.142976	-0.026778	2.993324
133.445469	2969.431097	6.147981	-0.026837	2.997110
133.720603	2977.482175	6.152986	-0.026893	3.000918
133.908591	2985.465206	6.157990	-0.026934	3.004684
134.054286	2993.521964	6.162995	-0.026966	3.008478
134.156348	3001.589570	6.168000	-0.026990	3.012271
134.296712	3009.620076	6.173005	-0.027022	3.016043
134.787008	3017.642744	6.178010	-0.027118	3.019823
134.883300	3025.674837	6.183014	-0.027141	3.023584
135.031502	3033.726285	6.188019	-0.027174	3.027352
135.321435	3041.748309	6.193024	-0.027234	3.031109
135.555603	3049.800991	6.198029	-0.027282	3.034872
135.654458	3057.852999	6.203034	-0.027306	3.038624
135.796517	3065.852065	6.208038	-0.027338	3.042348
136.141718	3073.877028	6.213043	-0.027407	3.046090
136.428953	3081.895115	6.218048	-0.027466	3.049821
136.481930	3089.967540	6.223053	-0.027481	3.053561
137.021151	3097.993840	6.228058	-0.027587	3.057299
136.937883	3106.032567	6.233062	-0.027577	3.061008
136.953339	3114.068868	6.238067	-0.027585	3.064717
137.241312	3122.127064	6.243072	-0.027644	3.068443
137.555316	3130.180340	6.248077	-0.027708	3.072165
137.805502	3138.271114	6.253082	-0.027759	3.075895
137.936005	3146.222069	6.258086	-0.027789	3.079552
138.235659	3154.236238	6.263091	-0.027850	3.083241
138.700000	3162.245541	6.268096	-0.027942	3.086931
138.865230	3170.278503	6.273101	-0.027978	3.090613
139.063498	3178.351991	6.278106	-0.028020	3.094311
139.215116	3186.389286	6.283110	-0.028054	3.097986
139.449307	3194.412838	6.288115	-0.028102	3.101654
139.796096	3202.425806	6.293120	-0.028172	3.105318
139.800848	3210.462723	6.298125	-0.028178	3.108973
140.128276	3218.531905	6.303130	-0.028245	3.112653
140.161061	3226.568564	6.308134	-0.028256	3.116300
140.638484	3234.567676	6.313139	-0.028350	3.119947
140.844900	3242.607440	6.318144	-0.028394	3.123595
140.821687	3250.621422	6.323149	-0.028395	3.127216
141.135410	3258.702691	6.328154	-0.028459	3.130879
141.235425	3266.737800	6.333158	-0.028482	3.134508
141.379200	3274.751616	6.338163	-0.028514	3.138124
141.550041	3282.772096	6.343168	-0.028552	3.141741
141.787243	3290.773853	6.348173	-0.028601	3.145348
142.223918	3298.835670	6.353178	-0.028688	3.148986
142.284367	3306.887374	6.358182	-0.028704	3.152599
142.650876	3314.910135	6.363187	-0.028778	3.156209
142.934996	3322.912584	6.368192	-0.028836	3.159801
142.940338	3330.949272	6.373197	-0.028842	3.163393
143.165807	3338.987061	6.378202	-0.028889	3.166990
143.577635	3346.992257	6.383206	-0.028971	3.170577
143.770201	3355.037021	6.388211	-0.029012	3.174168
144.060591	3363.089296	6.393216	-0.029072	3.177762
144.412009	3371.097166	6.398221	-0.029142	3.181335
144.881504	3379.134562	6.403226	-0.029235	3.184923
144.845298	3387.170503	6.408230	-0.029234	3.188484
145.303486	3395.204846	6.413235	-0.029324	3.192061
145.620260	3403.264045	6.418240	-0.029388	3.195639
145.680941	3411.253593	6.423245	-0.029405	3.199171
145.800496	3419.338429	6.428250	-0.029433	3.202745
146.119370	3427.340482	6.433254	-0.029497	3.206285
146.305721	3435.345639	6.438259	-0.029537	3.209818
146.400059	3443.445808	6.443264	-0.029560	3.213385
146.523373	3451.444948	6.448269	-0.029588	3.216905
146.688428	3459.471768	6.453274	-0.029624	3.220435
146.723484	3467.518254	6.458278	-0.029636	3.223964
147.005038	3475.527677	6.463283	-0.029694	3.227483
147.404437	3483.580677	6.468288	-0.029773	3.231022
147.149212	3491.688019	6.473293	-0.029731	3.234554
147.499455	3499.679786	6.478298	-0.029802	3.238057
147.829885	3507.662164	6.483302	-0.029868	3.241551
148.259210	3515.619774	6.488307	-0.029954	3.245034
148.382211	3523.681963	6.493312	-0.029982	3.248546
148.602515	3531.705875	6.498317	-0.030028	3.252043
148.863832	3539.775053	6.503322	-0.030082	3.255556
149.085746	3547.773147	6.508326	-0.030129	3.259033
149.440708	3555.782844	6.513331	-0.030200	3.262517
149.875217	3563.808443	6.518336	-0.030286	3.266007
149.749162	3571.844878	6.523341	-0.030268	3.269476
150.021337	3579.940328	6.528346	-0.030324	3.272982
150.349518	3587.977952	6.533350	-0.030390	3.276462
150.596184	3595.940336	6.538355	-0.030441	3.279903
150.797102	3603.979212	6.543360	-0.030484	3.283371
150.959841	3612.012703	6.548365	-0.030520	3.286831
151.388868	3620.040203	6.553370	-0.030605	3.290295
151.453941	3628.129492	6.558374	-0.030622	3.293769
151.681072	3636.126819	6.563379	-0.030670	3.297205
151.967108	3644.173294	6.568384	-0.030728	3.300661
152.076471	3652.157222	6.573389	-0.030754	3.304080
152.241559	3660.200805	6.578394	-0.030790	3.307523
152.322239	3668.269879	6.583398	-0.030810	3.310970
152.745897	3676.304512	6.588403	-0.030894	3.314412
152.914534	3684.314555	6.593408	-0.030931	3.317830
152.860261	3692.336492	6.598413	-0.030926	3.321241
153.198450	3700.329114	6.603418	-0.030994	3.324651
153.222258	3708.366597	6.608422	-0.031004	3.328064
153.454369	3716.400692	6.613427	-0.031053	3.331481
153.725950	3724.464024	6.618432	-0.031109	3.334907
153.609573	3732.497372	6.623437	-0.031092	3.338303
153.781463	3740.506329	6.628442	-0.031129	3.341696
154.137546	3748.509708	6.633446	-0.031201	3.345090
154.387320	3756.549867	6.638451	-0.031253	3.348492
154.507495	3764.614740	6.643456	-0.031280	3.351897
154.739252	3772.618898	6.648461	-0.031329	3.355276
154.950512	3780.607022	6.653466	-0.031373	3.358644
155.021376	3788.654742	6.658470	-0.031392	3.362029
155.449518	3796.654651	6.663475	-0.031477	3.365403
155.780476	3804.691975	6.668480	-0.031544	3.368786
155.776708	3812.745270	6.673485	-0.031548	3.372161
155.985222	3820.803464	6.678490	-0.031592	3.375541
156.082560	3828.821035	6.683494	-0.031616	3.378897
156.384071	3836.817341	6.688499	-0.031677	3.382248
156.738326	3844.845703	6.693504	-0.031748	3.385611
156.486061	3852.896745	6.698509	-0.031707	3.388959
156.937242	3860.994595	6.703514	-0.031796	3.392348
157.154028	3869.024382	6.708518	-0.031842	3.395696
157.146799	3877.011113	6.713523	-0.031846	3.399016
157.680898	3884.996454	6.718528	-0.031950	3.402351
157.900715	3892.983754	6.723533	-0.031996	3.405672
157.958082	3901.021886	6.728538	-0.032012	3.409005
158.063640	3909.075231	6.733542	-0.032037	3.412343
158.272676	3917.107550	6.738547	-0.032082	3.415673
158.586871	3925.095273	6.743552	-0.032145	3.418984
158.781525	3933.131023	6.748557	-0.032187	3.422308
159.213950	3941.134661	6.753562	-0.032273	3.425624
159.334283	3949.202978	6.758566	-0.032300	3.428952
159.397656	3957.250477	6.763571	-0.032317	3.432267
159.781548	3965.276553	6.768576	-0.032394	3.435580
159.872847	3973.264476	6.773581	-0.032416	3.438865
160.074574	3981.296765	6.778586	-0.032459	3.442168
160.179220	3989.348558	6.783590	-0.032484	3.445473
160.317341	3997.357391	6.788595	-0.032515	3.448759
160.643622	4005.406055	6.793600	-0.032581	3.452063
160.842637	4013.408671	6.798605	-0.032623	3.455342
161.212781	4021.448056	6.803610	-0.032697	3.458638
161.444567	4029.484951	6.808614	-0.032746	3.461925
161.341634	4037.513469	6.813619	-0.032732	3.465194
161.716132	4045.551310	6.818624	-0.032807	3.468480
161.995492	4053.581500	6.823629	-0.032864	3.471757
162.159665	4061.617033	6.828634	-0.032900	3.475029
162.099131	4069.638799	6.833638	-0.032894	3.478285
162.571978	4077.616677	6.838643	-0.032987	3.481537
162.906284	4085.633194	6.843648	-0.033055	3.484797
162.883521	4093.660776	6.848653	-0.033056	3.488048
163.296501	4101.711073	6.853658	-0.033138	3.491318
163.522442	4109.741250	6.858662	-0.033185	3.494571
163.673354	4117.740792	6.863667	-0.033219	3.497806
163.793676	4125.816001	6.868672	-0.033247	3.501068
163.875022	4133.795672	6.873677	-0.033267	3.504287
164.364381	4141.824027	6.878682	-0.033363	3.507536
164.446600	4149.865120	6.883686	-0.033384	3.510774
164.477243	4157.899783	6.888691	-0.033395	3.514004
164.874832	4165.923765	6.893696	-0.033474	3.517239
164.914076	4173.929864	6.898701	-0.033487	3.520452
165.100233	4181.938301	6.903706	-0.033527	3.523668
165.253752	4189.971454	6.908710	-0.033560	3.526890
165.583578	4197.980661	6.913715	-0.033627	3.530105
165.777767	4206.048251	6.918720	-0.033669	3.533336
165.966531	4214.075245	6.923725	-0.033709	3.536548
166.345550	4222.097612	6.928730	-0.033785	3.539760
166.465290	4230.125821	6.933734	-0.033812	3.542964
166.702679	4238.137622	6.938739	-0.033862	3.546162
166.936195	4246.163341	6.943744	-0.033911	3.549363
167.011736	4254.278144	6.948749	-0.033930	3.552591
167.128428	4262.354054	6.953754	-0.033957	3.555803
167.267125	4270.306615	6.958758	-0.033988	3.558963
167.238629	4278.288163	6.963763	-0.033988	3.562127
167.494265	4286.295999	6.968768	-0.034041	3.565306
167.837617	4294.288066	6.973773	-0.034110	3.568480
168.137178	4302.332494	6.978778	-0.034171	3.571669
168.242204	4310.384299	6.983782	-0.034196	3.574854
168.544114	4318.379081	6.988787	-0.034257	3.578018
168.677932	4326.445623	6.993792	-0.034288	3.581203
168.922470	4334.368669	6.998797	-0.034338	3.584332
169.086211	4342.464094	7.003802	-0.034374	3.587524
169.609836	4350.485169	7.008806	-0.034477	3.590693
169.767682	4358.494681	7.013811	-0.034512	3.593845
169.877776	4366.565654	7.018816	-0.034537	3.597017
169.805045	4374.550243	7.023821	-0.034529	3.600147
170.061737	4382.563588	7.028826	-0.034582	3.603295
170.294803	4390.612870	7.033830	-0.034631	3.606454
170.426049	4398.591153	7.038835	-0.034660	3.609579
170.661952	4406.656874	7.043840	-0.034710	3.612738
170.926090	4414.679786	7.048845	-0.034764	3.615879
171.098553	4422.685861	7.053850	-0.034801	3.619008
171.339744	4430.700515	7.058854	-0.034852	3.622139
171.468902	4438.714056	7.063859	-0.034881	3.625265
171.689037	4446.801231	7.068864	-0.034927	3.628418
171.874826	4454.795137	7.073869	-0.034967	3.631532
172.112212	4462.859927	7.078874	-0.035017	3.634671
172.306006	4470.883339	7.083878	-0.035058	3.637791
172.309233	4478.884255	7.088883	-0.035064	3.640895
172.643798	4486.852995	7.093888	-0.035131	3.643992
172.796213	4494.887199	7.098893	-0.035165	3.647106
173.040493	4502.932533	7.103898	-0.035216	3.650225
173.143530	4510.998580	7.108902	-0.035240	3.653346
173.410279	4519.035323	7.113907	-0.035295	3.656456
173.658015	4527.028527	7.118912	-0.035347	3.659547
173.862069	4535.051016	7.123917	-0.035390	3.662646
173.904668	4543.079168	7.128922	-0.035403	3.665739
174.040495	4551.111078	7.133926	-0.035434	3.668834
174.250212	4559.124558	7.138931	-0.035478	3.671921
174.448518	4567.172474	7.143936	-0.035520	3.675018
174.646140	4575.150031	7.148941	-0.035562	3.678086
174.942882	4583.183911	7.153946	-0.035623	3.681175
175.053295	4591.163735	7.158950	-0.035648	3.684236
175.482794	4599.217165	7.163955	-0.035734	3.687331
175.722675	4607.239494	7.168960	-0.035784	3.690407
175.776936	4615.281691	7.173965	-0.035799	3.693482
176.101985	4623.319354	7.178970	-0.035865	3.696561
176.421979	4631.304459	7.183974	-0.035930	3.699616
176.321514	4639.323804	7.188979	-0.035916	3.702672
176.756185	4647.370594	7.193984	-0.036002	3.705749
176.753564	4655.399365	7.198989	-0.036007	3.708805
176.928344	4663.465967	7.203994	-0.036045	3.711878
177.086358	4671.546996	7.208998	-0.036080	3.714953
177.223366	4679.499621	7.214003	-0.036110	3.717976
177.408242	4687.510863	7.219008	-0.036150	3.721020
177.494595	4695.441147	7.224013	-0.036171	3.724029
177.902555	4703.481035	7.229018	-0.036253	3.727085
178.054774	4711.529953	7.234022	-0.036286	3.730135
177.960617	4719.577213	7.239027	-0.036274	3.733176
178.418319	4727.604367	7.244032	-0.036365	3.736220
178.703606	4735.554018	7.249037	-0.036423	3.739229
178.824014	4743.627362	7.254042	-0.036451	3.742277
178.949749	4751.645703	7.259046	-0.036479	3.745303
179.293812	4759.647831	7.264051	-0.036549	3.748325
179.427233	4767.719487	7.269056	-0.036579	3.751366
179.594604	4775.728373	7.274061	-0.036615	3.754381
179.877050	4783.767415	7.279066	-0.036673	3.757408
180.156909	4791.774963	7.284070	-0.036730	3.760421
180.059264	4799.755657	7.289075	-0.036717	3.763413
180.324092	4807.847104	7.294080	-0.036772	3.766451
180.593677	4815.825666	7.299085	-0.036827	3.769446
180.754309	4823.884936	7.304090	-0.036863	3.772465
180.954175	4831.917454	7.309094	-0.036905	3.775473
181.351189	4839.896058	7.314099	-0.036984	3.778463
181.476742	4847.973668	7.319104	-0.037013	3.781482
181.597666	4855.925781	7.324109	-0.037041	3.784451
182.001047	4863.952742	7.329114	-0.037121	3.787452
182.291817	4872.016462	7.334118	-0.037181	3.790461
182.550309	4880.054235	7.339123	-0.037234	3.793458
183.013527	4888.122456	7.344128	-0.037325	3.796468
182.960865	4896.039500	7.349133	-0.037321	3.799409
183.005051	4904.067159	7.354138	-0.037334	3.802390
183.180926	4912.097617	7.359142	-0.037372	3.805373
183.226901	4920.100779	7.364147	-0.037386	3.808340
183.488717	4928.184468	7.369152	-0.037440	3.811340
183.452858	4936.147652	7.374157	-0.037439	3.814286
183.677486	4944.186339	7.379162	-0.037486	3.817263
183.914191	4952.206197	7.384166	-0.037535	3.820232
183.958689	4960.193564	7.389171	-0.037549	3.823182
184.259285	4968.241846	7.394176	-0.037610	3.826157
184.512651	4976.243314	7.399181	-0.037662	3.829112
184.727238	4984.291447	7.404186	-0.037708	3.832081
184.851529	4992.306927	7.409190	-0.037736	3.835034
185.114306	5000.325900	7.414195	-0.037790	3.837989
185.309769	5008.373668	7.419200	-0.037832	3.840950
185.336791	5016.335148	7.424205	-0.037842	3.843874
185.571543	5024.374483	7.429210	-0.037891	3.846829
185.865064	5032.381902	7.434214	-0.037951	3.849771
186.049730	5040.419539	7.439219	-0.037991	3.852719
186.093515	5048.501946	7.444224	-0.038004	3.855679
186.280091	5056.487926	7.449229	-0.038044	3.858604
186.562806	5064.517483	7.454234	-0.038102	3.861545
186.609139	5072.526924	7.459238	-0.038116	3.864471
186.674270	5080.580800	7.464243	-0.038133	3.867411
186.910047	5088.615274	7.469248	-0.038183	3.870346
187.116550	5096.821248	7.474253	-0.038226	3.873340
187.278901	5104.842205	7.479258	-0.038262	3.876264
187.440421	5112.741439	7.484262	-0.038297	3.879141
187.440624	5120.734307	7.489267	-0.038302	3.882047
187.917097	5128.724023	7.494272	-0.038396	3.884959
188.136465	5136.697517	7.499277	-0.038442	3.887858
188.276436	5144.738965	7.504282	-0.038474	3.890778
188.228697	5152.799040	7.509286	-0.038470	3.893698
188.384543	5160.803544	7.514291	-0.038505	3.896601
188.757540	5168.772481	7.519296	-0.038579	3.899492
188.747328	5176.833186	7.524301	-0.038583	3.902407
188.939682	5184.837506	7.529306	-0.038624	3.905303
189.265150	5192.841807	7.534310	-0.038689	3.908200
189.204348	5200.876511	7.539315	-0.038683	3.911098
189.536353	5208.948007	7.544320	-0.038751	3.914015
189.588026	5216.924786	7.549325	-0.038765	3.916890
189.920356	5224.869674	7.554330	-0.038833	3.919756
189.856988	5232.941394	7.559334	-0.038826	3.922659
190.129260	5240.930794	7.564339	-0.038882	3.925536
190.447653	5248.980355	7.569344	-0.038947	3.928434
190.437098	5257.000377	7.574349	-0.038950	3.931313
190.673429	5265.022595	7.579354	-0.038999	3.934195
190.869687	5273.086787	7.584358	-0.039041	3.937089
190.850572	5281.041299	7.589363	-0.039043	3.939937
191.171922	5289.069316	7.594368	-0.039108	3.942817
191.460908	5297.043819	7.599373	-0.039167	3.945674
191.610602	5305.095754	7.604378	-0.039200	3.948554
191.665017	5313.157436	7.609382	-0.039215	3.951434
191.837176	5321.186901	7.614387	-0.039253	3.954303
192.195026	5329.224630	7.619392	-0.039325	3.957175
192.207854	5337.180779	7.624397	-0.039332	3.960011
192.248095	5345.193942	7.629402	-0.039345	3.962865
192.604530	5353.190691	7.634406	-0.039417	3.965716
192.820734	5361.177228	7.639411	-0.039462	3.968560
192.957352	5369.297320	7.644416	-0.039493	3.971448
193.110099	5377.315310	7.649421	-0.039526	3.974297
193.478218	5385.300777	7.654426	-0.039600	3.977136
193.353131	5393.333832	7.659430	-0.039582	3.979982
193.610563	5401.326448	7.664435	-0.039635	3.982818
193.993858	5409.392218	7.669440	-0.039712	3.985680
194.079410	5417.390404	7.674445	-0.039733	3.988511
194.099571	5425.437097	7.679450	-0.039742	3.991357
194.391812	5433.443410	7.684454	-0.039802	3.994190
194.523240	5441.489461	7.689459	-0.039832	3.997032
194.582053	5449.526030	7.694464	-0.039848	3.999868
194.698941	5457.504563	7.699469	-0.039875	4.002683
195.048624	5465.503039	7.704474	-0.039945	4.005506
195.258233	5473.543799	7.709478	-0.039990	4.008340
195.419667	5481.587184	7.714483	-0.040025	4.011172
195.613725	5489.665965	7.719488	-0.040066	4.014015
195.643092	5497.657432	7.724493	-0.040077	4.016822
195.840813	5505.632806	7.729498	-0.040119	4.019625
196.187968	5513.657098	7.734502	-0.040189	4.022445
196.378121	5521.650419	7.739507	-0.040230	4.025250
196.619122	5529.719396	7.744512	-0.040280	4.028080
196.810616	5537.722259	7.749517	-0.040321	4.030884
197.238594	5545.843740	7.754522	-0.040406	4.033731
197.241259	5553.855488	7.759526	-0.040412	4.036532
197.580216	5561.748375	7.764531	-0.040480	4.039294
197.841409	5569.796878	7.769536	-0.040534	4.042107
198.048590	5577.782671	7.774541	-0.040578	4.044896
198.011394	5585.828335	7.779546	-0.040576	4.047700
198.058854	5593.859858	7.784550	-0.040590	4.050498
198.483464	5601.869451	7.789555	-0.040674	4.053292
198.670601	5609.919828	7.794560	-0.040714	4.056095
198.651312	5617.860462	7.799565	-0.040716	4.058855
198.857658	5625.920326	7.804570	-0.040760	4.061657
199.101940	5633.905112	7.809574	-0.040811	4.064433
199.121306	5641.954213	7.814579	-0.040819	4.067225
199.495884	5649.958314	7.819584	-0.040894	4.070005
199.818222	5658.007139	7.824589	-0.040960	4.072797
199.950919	5666.042237	7.829594	-0.040990	4.075581
200.082252	5674.033290	7.834598	-0.041019	4.078347
200.132297	5682.041217	7.839603	-0.041034	4.081116
200.518959	5690.039381	7.844608	-0.041111	4.083884
200.384492	5698.076484	7.849613	-0.041091	4.086657
200.700369	5706.051423	7.854618	-0.041156	4.089412
200.902665	5714.130557	7.859622	-0.041198	4.092200
200.754409	5722.132905	7.864627	-0.041176	4.094955
200.969983	5730.157277	7.869632	-0.041222	4.097720
201.180088	5738.164684	7.874637	-0.041266	4.100478
201.312838	5746.158755	7.879642	-0.041296	4.103228
201.382833	5754.215195	7.884646	-0.041314	4.105997
201.739820	5762.215231	7.889651	-0.041386	4.108749
201.948968	5770.312864	7.894656	-0.041430	4.111530
202.099382	5778.323562	7.899661	-0.041463	4.114278
202.186236	5786.323844	7.904666	-0.041485	4.117021
202.405374	5794.321827	7.909670	-0.041531	4.119762
202.646744	5802.322585	7.914675	-0.041581	4.122503
202.822281	5810.337599	7.919680	-0.041619	4.125246
202.904296	5818.343188	7.924685	-0.041640	4.127983
202.999783	5826.429544	7.929690	-0.041663	4.130745
203.343697	5834.455587	7.934694	-0.041732	4.133489
203.581289	5842.461654	7.939699	-0.041781	4.136222
203.696574	5850.445450	7.944704	-0.041808	4.138944
203.700703	5858.495387	7.949709	-0.041814	4.141686
204.058684	5866.450904	7.954714	-0.041886	4.144398
204.282119	5874.549686	7.959718	-0.041933	4.147155
204.213100	5882.525515	7.964723	-0.041925	4.149866
204.544436	5890.597332	7.969728	-0.041992	4.152611
204.811884	5898.591300	7.974733	-0.042047	4.155328
204.830757	5906.598301	7.979738	-0.042056	4.158045
204.939372	5914.646155	7.984742	-0.042082	4.160774
205.051573	5922.594136	7.989747	-0.042108	4.163468
205.512004	5930.624019	7.994752	-0.042199	4.166192
205.463490	5938.643347	7.999757	-0.042195	4.168905
205.574583	5946.713316	8.004762	-0.042221	4.171635
205.939042	5954.733938	8.009766	-0.042294	4.174349
205.995269	5962.757239	8.014771	-0.042310	4.177059
206.329256	5970.741431	8.019776	-0.042377	4.179757
206.504982	5978.754648	8.024781	-0.042415	4.182461
206.641685	5986.760506	8.029786	-0.042446	4.185161
206.765379	5994.808183	8.034790	-0.042474	4.187873
206.929631	6002.783739	8.039795	-0.042510	4.190559
207.175029	6010.969864	8.044800	-0.042561	4.193315
207.127718	6018.952480	8.049805	-0.042558	4.195998
207.379226	6026.856347	8.054810	-0.042610	4.198655
207.530090	6034.921999	8.059814	-0.042643	4.201365
207.647895	6042.821747	8.064819	-0.042670	4.204016
207.833561	6050.921900	8.069824	-0.042710	4.206734
208.173311	6058.850175	8.074829	-0.042778	4.209394
208.264589	6066.948867	8.079834	-0.042801	4.212106
208.410015	6074.977443	8.084838	-0.042833	4.214795
208.690323	6082.942681	8.089843	-0.042891	4.217461
208.971075	6090.990631	8.094848	-0.042948	4.220153
208.932829	6098.995420	8.099853	-0.042946	4.222826
209.068410	6107.030043	8.104858	-0.042977	4.225510
209.367382	6115.066879	8.109862	-0.043038	4.228193
209.291387	6123.026272	8.114867	-0.043029	4.230846
209.481513	6131.143182	8.119872	-0.043070	4.233552
209.551988	6139.126250	8.124877	-0.043088	4.236210
209.778272	6147.092050	8.129882	-0.043135	4.238862
209.832948	6155.150499	8.134886	-0.043151	4.241542
210.032554	6163.111275	8.139891	-0.043193	4.244189
210.286472	6171.168683	8.144896	-0.043246	4.246867
210.330948	6179.207038	8.149901	-0.043259	4.249536
210.680903	6187.206195	8.154906	-0.043330	4.252192
210.860808	6195.271733	8.159910	-0.043368	4.254867
211.067095	6203.254963	8.164915	-0.043412	4.257513
211.110377	6211.290142	8.169920	-0.043425	4.260173
211.176830	6219.299534	8.174925	-0.043443	4.262823
211.408989	6227.316112	8.179930	-0.043492	4.265476
211.383723	6235.370158	8.184934	-0.043492	4.268137
211.475378	6243.372226	8.189939	-0.043514	4.270780
211.809262	6251.449595	8.194944	-0.043582	4.273448
211.877766	6259.471834	8.199949	-0.043600	4.276094
212.066832	6267.404996	8.204954	-0.043640	4.278711
212.462186	6275.480024	8.209958	-0.043719	4.281374
212.344537	6283.394001	8.214963	-0.043703	4.283978
212.767959	6291.443375	8.219968	-0.043787	4.286629
212.989526	6299.462128	8.224973	-0.043833	4.289267
213.236727	6307.462464	8.229978	-0.043884	4.291898
213.429085	6315.540503	8.234982	-0.043926	4.294552
213.382601	6323.519079	8.239987	-0.043922	4.297170
213.726926	6331.539674	8.244992	-0.043992	4.299803
213.778582	6339.555234	8.249997	-0.044006	4.302430
213.757977	6347.565056	8.255002	-0.044008	4.305054
214.099752	6355.633182	8.260006	-0.044077	4.307698
214.195264	6363.581419	8.265011	-0.044100	4.310298
214.450410	6371.684567	8.270016	-0.044153	4.312950
214.441730	6379.700466	8.275021	-0.044156	4.315569
214.670963	6387.662226	8.280026	-0.044204	4.318170
214.928928	6395.700963	8.285030	-0.044257	4.320796
214.874303	6403.647375	8.290035	-0.044252	4.323387
215.163284	6411.709667	8.295040	-0.044312	4.326017
215.382529	6419.718136	8.300045	-0.044358	4.328627
215.541649	6427.741488	8.305050	-0.044393	4.331240
215.877520	6435.797587	8.310054	-0.044460	4.333864
216.122026	6443.849156	8.315059	-0.044511	4.336483
216.171634	6451.776280	8.320064	-0.044526	4.339060
216.143603	6459.879033	8.325069	-0.044526	4.341691
216.362072	6467.765027	8.330074	-0.044572	4.344252
216.619915	6475.860986	8.335078	-0.044625	4.346880
216.761216	6483.863202	8.340083	-0.044656	4.349475
217.190374	6491.935721	8.345088	-0.044742	4.352093
217.171085	6500.048386	8.350093	-0.044743	4.354719
217.222009	6507.981171	8.355098	-0.044758	4.357286
217.480303	6515.948351	8.360102	-0.044811	4.359865
217.567671	6523.947868	8.365107	-0.044833	4.362451
217.709346	6531.940484	8.370112	-0.044865	4.365033
217.755567	6539.966822	8.375117	-0.044878	4.367624
217.875745	6547.933624	8.380122	-0.044906	4.370195
218.185300	6556.038174	8.385126	-0.044969	4.372810
218.037728	6564.028304	8.390131	-0.044947	4.375384
218.443755	6572.025475	8.395136	-0.045028	4.377962
218.560298	6580.042520	8.400141	-0.045055	4.380543
218.607864	6588.036467	8.405146	-0.045069	4.383114
218.822268	6596.080726	8.410150	-0.045114	4.385702
218.889544	6604.102297	8.415155	-0.045132	4.388279
218.998695	6612.135667	8.420160	-0.045157	4.390859
219.128647	6620.161776	8.425165	-0.045187	4.393436
219.309152	6628.183027	8.430170	-0.045226	4.396009
219.551556	6636.199244	8.435174	-0.045276	4.398580
219.494101	6644.183342	8.440179	-0.045271	4.401137
219.495349	6652.176952	8.445184	-0.045276	4.403696
219.796534	6660.210344	8.450189	-0.045337	4.406268
219.898820	6668.221489	8.455194	-0.045362	4.408830
220.115907	6676.285351	8.460198	-0.045407	4.411408
220.402628	6684.311863	8.465203	-0.045466	4.413973
220.640784	6692.366423	8.470208	-0.045516	4.416546
220.727571	6700.322380	8.475213	-0.045537	4.419084
220.899753	6708.363936	8.480218	-0.045574	4.421649
221.115740	6716.330198	8.485222	-0.045620	4.424188
221.145370	6724.396060	8.490227	-0.045631	4.426757
221.437998	6732.411774	8.495232	-0.045690	4.429310
221.512905	6740.423583	8.500237	-0.045710	4.431858
221.544580	6748.436725	8.505242	-0.045721	4.434406
221.720750	6756.521279	8.510246	-0.045759	4.436975
221.744414	6764.473046	8.515251	-0.045768	4.439500
222.115436	6772.516151	8.520256	-0.045843	4.442054
222.040903	6780.484348	8.525261	-0.045834	4.444581
222.179247	6788.552765	8.530266	-0.045865	4.447140
222.578687	6796.545606	8.535270	-0.045945	4.449673
222.453791	6804.576517	8.540275	-0.045927	4.452216
222.652049	6812.593097	8.545280	-0.045969	4.454753
223.048998	6820.623714	8.550285	-0.046048	4.457295
223.061233	6828.599563	8.555290	-0.046056	4.459816
223.251612	6836.651937	8.560295	-0.046096	4.462360
223.395118	6844.592825	8.565299	-0.046128	4.464868
223.636042	6852.687544	8.570304	-0.046179	4.467423
223.704424	6860.662220	8.575309	-0.046197	4.469938
223.714217	6868.737202	8.580314	-0.046204	4.472483
224.096508	6876.764096	8.585319	-0.046280	4.475013
224.238637	6884.716959	8.590323	-0.046312	4.477517
224.380640	6892.713047	8.595328	-0.046343	4.480033
224.403421	6900.759634	8.600333	-0.046353	4.482563
224.514134	6908.698589	8.605338	-0.046379	4.485059
224.727906	6916.766249	8.610343	-0.046424	4.487594
224.778963	6924.788444	8.615347	-0.046439	4.490112
224.948256	6932.846871	8.620352	-0.046476	4.492641
225.041047	6940.853872	8.625357	-0.046498	4.495152
225.292692	6948.856941	8.630362	-0.046550	4.497661
225.496910	6956.855048	8.635367	-0.046593	4.500166
225.336939	6964.846982	8.640371	-0.046569	4.502668
225.693340	6972.860758	8.645376	-0.046641	4.505176
225.976492	6980.911733	8.650381	-0.046699	4.507694
226.193212	6988.922916	8.655386	-0.046744	4.510198
226.419839	6997.045547	8.660391	-0.046792	4.512736
226.398142	7005.007752	8.665395	-0.046793	4.515221
226.504556	7013.037412	8.670400	-0.046818	4.517727
226.563173	7020.957766	8.675405	-0.046834	4.520197
226.854410	7028.958932	8.680410	-0.046894	4.522691
227.290191	7036.980645	8.685415	-0.046980	4.525190
227.260232	7045.013230	8.690419	-0.046980	4.527691
227.285347	7053.021772	8.695424	-0.046990	4.530182
227.586523	7061.065062	8.700429	-0.047051	4.532684
227.681152	7069.055959	8.705434	-0.047074	4.535168
227.869243	7077.118065	8.710439	-0.047114	4.537672
228.068748	7085.100137	8.715443	-0.047156	4.540150
228.303101	7093.118662	8.720448	-0.047205	4.542639
228.333720	7101.111607	8.725453	-0.047216	4.545117
228.478538	7109.119399	8.730458	-0.047249	4.547599
228.749995	7117.173315	8.735463	-0.047304	4.550094
228.709909	7125.194999	8.740467	-0.047302	4.552577
229.007715	7133.235571	8.745472	-0.047363	4.555066
229.117579	7141.230032	8.750477	-0.047389	4.557538
229.113776	7149.244546	8.755482	-0.047393	4.560015
229.176196	7157.261121	8.760487	-0.047410	4.562491
229.338607	7165.219976	8.765491	-0.047445	4.564949
229.707771	7173.277527	8.770496	-0.047520	4.567435
229.460430	7181.284160	8.775501	-0.047479	4.569904
229.738234	7189.313476	8.780506	-0.047536	4.572379
230.095769	7197.355109	8.785511	-0.047608	4.574857
230.117563	7205.376924	8.790515	-0.047617	4.577327
230.190516	7213.348140	8.795520	-0.047636	4.579780
230.382995	7221.406606	8.800525	-0.047677	4.582258
230.510405	7229.395517	8.805530	-0.047706	4.584714
230.640657	7237.500577	8.810535	-0.047735	4.587204
230.771059	7245.428048	8.815539	-0.047765	4.589638
230.978133	7253.508207	8.820544	-0.047809	4.592118
231.281938	7261.526478	8.825549	-0.047871	4.594578
231.396137	7269.569834	8.830554	-0.047897	4.597043
231.705012	7277.486839	8.835559	-0.047960	4.599469
231.720534	7285.571650	8.840563	-0.047968	4.601945
231.654885	7293.508873	8.845568	-0.047961	4.604374
231.845441	7301.570544	8.850573	-0.048002	4.606840
232.045400	7309.542640	8.855578	-0.048044	4.609278
232.100354	7317.626400	8.860583	-0.048060	4.611748
232.174411	7325.604087	8.865587	-0.048079	4.614184
232.463068	7333.668905	8.870592	-0.048138	4.616646
232.506987	7341.664389	8.875597	-0.048151	4.619085
232.520895	7349.671281	8.880602	-0.048159	4.621527
232.930180	7357.658072	8.885607	-0.048241	4.623960
232.928216	7365.678636	8.890611	-0.048245	4.626403
233.068700	7373.674867	8.895616	-0.048277	4.628838
233.438912	7381.754676	8.900621	-0.048351	4.631296
233.543052	7389.767701	8.905626	-0.048376	4.633733
233.676136	7397.827164	8.910631	-0.048406	4.636182
233.795314	7405.750089	8.915635	-0.048433	4.638589
234.164592	7413.782589	8.920640	-0.048507	4.641028
234.231168	7421.764263	8.925645	-0.048525	4.643450
234.239525	7429.800453	8.930650	-0.048532	4.645887
234.342827	7437.843177	8.935655	-0.048556	4.648325
234.546133	7445.817268	8.940659	-0.048599	4.650741
234.656063	7453.867503	8.945664	-0.048625	4.653178
234.699280	7461.899100	8.950669	-0.048638	4.655609
234.937855	7469.878795	8.955674	-0.048688	4.658023
235.164739	7477.927758	8.960679	-0.048736	4.660456
235.242676	7485.912262	8.965683	-0.048755	4.662869
235.390322	7493.935333	8.970688	-0.048788	4.665292
235.731519	7501.929301	8.975693	-0.048857	4.667704
235.605769	7509.934842	8.980698	-0.048839	4.670120
235.886809	7518.079915	8.985703	-0.048896	4.672576
236.222248	7526.102202	8.990707	-0.048964	4.674993
236.261739	7534.052686	8.995712	-0.048977	4.677388
236.252509	7542.023615	9.000717	-0.048980	4.679788
236.290372	7550.027946	9.005722	-0.048992	4.682196
236.552456	7558.020000	9.010727	-0.049046	4.684600
236.495696	7566.022766	9.015731	-0.049041	4.687006
236.665070	7574.050707	9.020736	-0.049078	4.689417
236.922099	7582.094825	9.025741	-0.049131	4.691832
237.091165	7590.076056	9.030746	-0.049168	4.694228
237.247791	7598.175863	9.035751	-0.049202	4.696657
237.312920	7606.084561	9.040755	-0.049220	4.699028
237.470139	7614.134424	9.045760	-0.049254	4.701440
237.736055	7622.117317	9.050765	-0.049309	4.703831
237.882912	7630.178624	9.055770	-0.049342	4.706244
238.069192	7638.226685	9.060775	-0.049382	4.708652
238.002201	7646.180945	9.065779	-0.049374	4.711031
238.140374	7654.268271	9.070784	-0.049405	4.713448
238.308038	7662.298375	9.075789	-0.049442	4.715846
238.673166	7670.266284	9.080794	-0.049515	4.718225
238.665010	7678.289633	9.085799	-0.049519	4.720619
238.835189	7686.267297	9.090803	-0.049556	4.722999
239.162625	7694.315381	9.095808	-0.049622	4.725397
239.173502	7702.350170	9.100813	-0.049629	4.727791
239.298261	7710.310405	9.105818	-0.049658	4.730162
239.346853	7718.430278	9.110823	-0.049672	4.732579
239.288081	7726.371729	9.115827	-0.049666	4.734942
239.506462	7734.372344	9.120832	-0.049712	4.737321
239.805419	7742.413595	9.125837	-0.049773	4.739710
239.782367	7750.426322	9.130842	-0.049774	4.742091
240.192422	7758.440199	9.135847	-0.049856	4.744469
240.496552	7766.492920	9.140851	-0.049918	4.746858
240.566587	7774.482036	9.145856	-0.049936	4.749227
240.817859	7782.546677	9.150861	-0.049988	4.751618
240.983614	7790.568163	9.155866	-0.050024	4.753994
241.286516	7798.582637	9.160871	-0.050086	4.756367
241.156398	7806.488648	9.165875	-0.050067	4.758708
241.242991	7814.522420	9.170880	-0.050088	4.761084
241.564275	7822.569379	9.175885	-0.050153	4.763463
241.517542	7830.551591	9.180890	-0.050150	4.765823
241.659064	7838.565433	9.185895	-0.050181	4.768190
241.706693	7846.608585	9.190899	-0.050196	4.770565
241.749427	7854.620792	9.195904	-0.050209	4.772929
241.948763	7862.688769	9.200909	-0.050251	4.775309
241.962619	7870.613330	9.205914	-0.050259	4.777645
242.320938	7878.670332	9.210919	-0.050331	4.780018
242.332102	7886.637754	9.215923	-0.050338	4.782365
242.476002	7894.638493	9.220928	-0.050370	4.784720
242.832419	7902.722589	9.225933	-0.050442	4.787097
242.941305	7910.711813	9.230938	-0.050468	4.789447
243.154081	7918.772350	9.235943	-0.050512	4.791815
243.355673	7926.771973	9.240947	-0.050555	4.794165
243.473657	7934.819040	9.245952	-0.050582	4.796528
243.504240	7942.717764	9.250957	-0.050593	4.798846
243.638487	7950.803894	9.255962	-0.050624	4.801218
243.816581	7958.773349	9.260967	-0.050662	4.803554
243.969818	7966.808172	9.265971	-0.050696	4.805908
243.967051	7974.833905	9.270976	-0.050701	4.808259
244.114232	7982.892607	9.275981	-0.050733	4.810618
244.280960	7990.404003	9.280986	-0.050769	4.812816
244.417745	7995.122942	9.285991	-0.050798	4.814196

244.400276	7997.588290	9.290995	-0.050796	4.814917
244.558685	7998.786447	9.296000	-0.050827	4.815267
244.665191	7999.656104	9.301005	-0.050847	4.815521
244.738564	7999.602850	9.306010	-0.050861	4.815505
244.743672	8000.108982	9.311015	-0.050862	4.815653
244.864628	8000.368248	9.316019	-0.050885	4.815728
244.774551	8000.269634	9.321024	-0.050868	4.815700
244.730832	8000.279603	9.326029	-0.050860	4.815703
244.840975	8000.245095	9.331034	-0.050880	4.815692
244.824773	8000.199995	9.336039	-0.050877	4.815679
244.791328	8000.238957	9.341043	-0.050871	4.815690
244.911994	8000.274016	9.346048	-0.050894	4.815700
244.989660	8000.236845	9.351053	-0.050908	4.815689
244.922320	8000.363872	9.356058	-0.050896	4.815726
245.182895	8000.156712	9.361063	-0.050944	4.815665
245.075994	8000.329006	9.366067	-0.050924	4.815715
245.026514	8000.128557	9.371072	-0.050915	4.815657
245.128675	8000.159045	9.376077	-0.050934	4.815665
245.031965	8000.391291	9.381082	-0.050916	4.815734
245.199148	8000.145248	9.386087	-0.050947	4.815661
245.007024	8000.145336	9.391091	-0.050912	4.815662
245.239442	8000.056227	9.396096	-0.050955	4.815635
245.449530	8000.149322	9.401101	-0.050994	4.815661
245.355289	8000.252425	9.406106	-0.050977	4.815692
245.446434	8000.143940	9.411111	-0.050994	4.815660
245.522963	8000.199636	9.416115	-0.051008	4.815675
245.442676	8000.058474	9.421120	-0.050993	4.815635
245.689987	8000.332608	9.426125	-0.051039	4.815714
245.597373	8000.225409	9.431130	-0.051022	4.815683
245.488929	8000.135037	9.436135	-0.051002	4.815657
245.548614	8000.250248	9.441139	-0.051013	4.815690
245.732102	7999.993792	9.446144	-0.051047	4.815614
245.824914	8000.112743	9.451149	-0.051064	4.815649
245.729696	8000.083441	9.456154	-0.051047	4.815641
245.851545	8000.139873	9.461159	-0.051069	4.815656
245.912083	8000.235880	9.466163	-0.051081	4.815684
245.903868	8000.132187	9.471168	-0.051079	4.815654
246.085958	8000.147959	9.476173	-0.051113	4.815658
246.068564	8000.174371	9.481178	-0.051110	4.815665
246.045607	7999.986095	9.486183	-0.051106	4.815611
245.881555	8000.094470	9.491187	-0.051075	4.815643
246.017236	8000.046496	9.496192	-0.051100	4.815628
246.133158	8000.217072	9.501197	-0.051122	4.815678
246.005556	8000.076207	9.506202	-0.051098	4.815637
246.068027	7999.971528	9.511207	-0.051110	4.815606
246.005496	8000.079416	9.516211	-0.051098	4.815638
246.000204	8000.128445	9.521216	-0.051097	4.815652
246.020611	8000.028420	9.526221	-0.051101	4.815623
245.984441	8000.201864	9.531226	-0.051095	4.815674
246.133279	7999.935235	9.536231	-0.051122	4.815595
246.065187	8000.097483	9.541235	-0.051110	4.815643
246.070984	8000.159505	9.546240	-0.051111	4.815661
246.100926	8000.029740	9.551245	-0.051116	4.815623
246.150536	8000.164006	9.556250	-0.051126	4.815662
246.337899	7999.953520	9.561255	-0.051161	4.815600
246.399174	8000.197945	9.566259	-0.051172	4.815671
246.266419	8000.069808	9.571264	-0.051147	4.815634
246.284506	8000.003910	9.576269	-0.051151	4.815615
246.325276	8000.178604	9.581274	-0.051158	4.815665
246.356393	7999.907927	9.586279	-0.051164	4.815586
246.036314	8000.215556	9.591283	-0.051105	4.815678
246.165137	7999.843973	9.596288	-0.051129	4.815568
246.322341	7999.971443	9.601293	-0.051158	4.815605
246.141490	8000.156417	9.606298	-0.051124	4.815660
246.132186	7999.997188	9.611303	-0.051123	4.815613
246.354653	8000.026427	9.616307	-0.051164	4.815621
246.307858	7999.979762	9.621312	-0.051155	4.815607
246.248938	8000.148566	9.626317	-0.051145	4.815657
246.358096	8000.110838	9.631322	-0.051165	4.815646
246.374996	7999.964846	9.636327	-0.051168	4.815603
246.080196	8000.086046	9.641331	-0.051113	4.815640
246.409853	7999.992110	9.646336	-0.051175	4.815611
246.275235	7999.999536	9.651341	-0.051150	4.815613
246.243429	8000.138886	9.656346	-0.051144	4.815654
246.316191	7999.953231	9.661351	-0.051157	4.815600
246.413046	8000.152324	9.666355	-0.051175	4.815657
246.359888	8000.074592	9.671360	-0.051165	4.815635
246.245059	7999.967032	9.676365	-0.051144	4.815604
246.256047	7999.990702	9.681370	-0.051146	4.815611
246.634760	7999.960555	9.686375	-0.051217	4.815600
246.573452	8000.018284	9.691379	-0.051205	4.815617
246.514592	8000.102744	9.696384	-0.051194	4.815642
246.494023	8000.085330	9.701389	-0.051191	4.815637
246.431402	8000.151580	9.706394	-0.051179	4.815657
246.509628	7999.857111	9.711399	-0.051194	4.815571
246.665469	7999.894877	9.716403	-0.051223	4.815581
246.608423	7999.872601	9.721408	-0.051212	4.815575
246.506504	8000.088752	9.726413	-0.051193	4.815638
246.525863	8000.108288	9.731418	-0.051197	4.815644
246.677291	7999.917503	9.736423	-0.051225	4.815587
246.546004	8000.013599	9.741427	-0.051201	4.815616
246.412089	7999.962315	9.746432	-0.051176	4.815602
246.837436	7999.984173	9.751437	-0.051255	4.815606
246.519082	8000.150900	9.756442	-0.051196	4.815656
246.576220	8000.050403	9.761447	-0.051206	4.815627
246.599136	8000.288869	9.766451	-0.051211	4.815696
246.585325	8000.009986	9.771456	-0.051208	4.815615
246.462544	8000.018672	9.776461	-0.051185	4.815618
246.528913	8000.080609	9.781466	-0.051198	4.815636
246.709662	7999.955428	9.786471	-0.051231	4.815598
246.803444	7999.984714	9.791475	-0.051249	4.815606
246.648340	8000.096438	9.796480	-0.051220	4.815640
246.605916	8000.006068	9.801485	-0.051212	4.815614
246.660529	8000.132943	9.806490	-0.051222	4.815651
246.573929	7999.939360	9.811495	-0.051206	4.815594
246.705452	8000.008762	9.816499	-0.051231	4.815614
246.766697	8000.097309	9.821504	-0.051242	4.815640
246.838689	8000.064316	9.826509	-0.051256	4.815630
246.799050	8000.009224	9.831514	-0.051248	4.815614
246.833618	7999.972420	9.836519	-0.051255	4.815603
246.912920	8000.126388	9.841523	-0.051270	4.815647
246.760368	8000.122846	9.846528	-0.051241	4.815647
246.885754	8000.134495	9.851533	-0.051265	4.815650
246.763935	8000.190174	9.856538	-0.051242	4.815667
246.742131	8000.106544	9.861543	-0.051238	4.815642
246.749579	8000.093856	9.866547	-0.051239	4.815639
246.919967	8000.084883	9.871552	-0.051271	4.815635
246.884559	8000.040536	9.876557	-0.051265	4.815622
246.766064	8000.089863	9.881562	-0.051243	4.815637
246.972000	7999.969361	9.886567	-0.051281	4.815601
246.955545	8000.034225	9.891571	-0.051278	4.815620
246.760797	7999.960599	9.896576	-0.051242	4.815600
246.741816	8000.080940	9.901581	-0.051238	4.815635
246.761497	8000.023609	9.906586	-0.051242	4.815618
246.906702	7999.889309	9.911591	-0.051269	4.815578
246.906523	8000.027038	9.916595	-0.051269	4.815618
246.906702	8000.024909	9.921600	-0.051269	4.815618
246.813524	7999.959339	9.926605	-0.051252	4.815599
246.769338	8000.102760	9.931610	-0.051244	4.815641
246.862265	8000.128829	9.936615	-0.051261	4.815648
246.738853	8000.220783	9.941619	-0.051238	4.815676
246.856405	8000.165041	9.946624	-0.051260	4.815659
247.008147	7999.951839	9.951629	-0.051288	4.815596
246.920799	7999.986724	9.956634	-0.051272	4.815606
246.839597	7999.987544	9.961639	-0.051257	4.815607
246.758084	8000.144238	9.966643	-0.051242	4.815653
246.998852	8000.109716	9.971648	-0.051287	4.815642
246.978713	7999.917211	9.976653	-0.051283	4.815586
246.871078	8000.089496	9.981658	-0.051263	4.815637
247.207093	7999.967904	9.986663	-0.051325	4.815600
247.094242	8000.156121	9.991667	-0.051305	4.815655
247.077356	8000.119549	9.996672	-0.051301	4.815645
246.975472	7999.973761	10.001677	-0.051282	4.815602
246.917510	8000.168207	10.006682	-0.051272	4.815660
247.018074	7999.883707	10.011687	-0.051290	4.815576
246.859289	8000.074380	10.016691	-0.051261	4.815632
247.081161	8000.026738	10.021696	-0.051302	4.815617
247.013071	7999.956237	10.026701	-0.051290	4.815597
246.788019	8000.172525	10.031706	-0.051248	4.815661
246.955306	7999.866689	10.036711	-0.051279	4.815571
247.056809	7999.987919	10.041715	-0.051298	4.815606
246.861215	7999.976204	10.046720	-0.051261	4.815604
246.979296	8000.024035	10.051725	-0.051284	4.815617
247.075970	8000.020270	10.056730	-0.051302	4.815616
247.060978	8000.026436	10.061735	-0.051299	4.815617
246.768325	8000.080407	10.066739	-0.051244	4.815635
247.039863	8000.146747	10.071744	-0.051295	4.815653
247.019329	8000.119724	10.076749	-0.051291	4.815645
246.981421	7999.966434	10.081754	-0.051284	4.815600
246.994269	8000.005082	10.086759	-0.051287	4.815611
247.080116	7999.988329	10.091763	-0.051303	4.815606
246.954648	7999.986294	10.096768	-0.051279	4.815606
247.222391	8000.021609	10.101773	-0.051329	4.815615
246.915925	7999.965386	10.106778	-0.051272	4.815600
247.282455	7999.852831	10.111783	-0.051340	4.815566
246.935928	7999.977462	10.116787	-0.051276	4.815604
247.093857	7999.965083	10.121792	-0.051305	4.815599
247.110422	8000.199177	10.126797	-0.051309	4.815668
247.103846	8000.083763	10.131802	-0.051307	4.815634
247.191522	7999.836422	10.136807	-0.051324	4.815561
247.118400	8000.043434	10.141811	-0.051310	4.815622
247.181912	7999.955852	10.146816	-0.051322	4.815596
247.471885	8000.024626	10.151821	-0.051376	4.815615
247.348880	8000.172107	10.156826	-0.051353	4.815659
247.260832	7999.958211	10.161831	-0.051337	4.815596
247.130955	7999.883503	10.166835	-0.051313	4.815575
247.095979	7999.985434	10.171840	-0.051306	4.815605
247.201693	7999.868643	10.176845	-0.051326	4.815571
247.155832	8000.168986	10.181850	-0.051317	4.815659
247.128099	7999.982763	10.186855	-0.051312	4.815604
247.061002	8000.040398	10.191859	-0.051300	4.815621
247.147908	8000.005512	10.196864	-0.051316	4.815611
247.181750	7999.974034	10.201869	-0.051322	4.815601
247.270547	8000.124955	10.206874	-0.051339	4.815645
247.496150	7999.969539	10.211879	-0.051381	4.815599
247.071955	7999.986140	10.216883	-0.051302	4.815606
247.142522	7999.941380	10.221888	-0.051315	4.815592
247.175170	7999.899206	10.226893	-0.051321	4.815580
247.146527	8000.085587	10.231898	-0.051316	4.815634
247.254600	7999.983781	10.236903	-0.051336	4.815604
247.410740	8000.010877	10.241907	-0.051365	4.815611
247.155609	7999.981112	10.246912	-0.051318	4.815604
247.163936	8000.068800	10.251917	-0.051319	4.815629
247.137601	8000.029939	10.256922	-0.051315	4.815618
247.224047	8000.133844	10.261927	-0.051331	4.815648
247.351326	8000.046229	10.266931	-0.051354	4.815622
247.329220	8000.108867	10.271936	-0.051350	4.815640
247.409019	8000.128317	10.276941	-0.051365	4.815646
247.407540	8000.031137	10.281946	-0.051365	4.815617
247.285384	8000.085743	10.286951	-0.051342	4.815634
247.258866	8000.136564	10.291955	-0.051337	4.815649
247.409209	8000.008752	10.296960	-0.051365	4.815611
247.387353	7999.969964	10.301965	-0.051361	4.815599
247.284328	8000.015271	10.306970	-0.051342	4.815613
247.509198	7999.897212	10.311975	-0.051384	4.815577
247.307138	7999.988956	10.316979	-0.051346	4.815605
247.347066	8000.097444	10.321984	-0.051354	4.815637
247.461594	7999.925275	10.326989	-0.051375	4.815586
247.380010	7999.982675	10.331994	-0.051360	4.815603
247.303986	7999.873608	10.336999	-0.051346	4.815572
247.386399	8000.044711	10.342003	-0.051361	4.815621
247.492796	8000.144671	10.347008	-0.051381	4.815650
247.276506	7999.885984	10.352013	-0.051341	4.815575
247.367970	7999.866119	10.357018	-0.051358	4.815569
247.492390	7999.876684	10.362023	-0.051381	4.815572
247.423590	8000.061347	10.367027	-0.051369	4.815626
247.388767	8000.097085	10.372032	-0.051362	4.815636
247.515900	8000.006265	10.377037	-0.051386	4.815609
247.406326	7999.984202	10.382042	-0.051365	4.815603
247.190550	8000.005257	10.387047	-0.051325	4.815611
247.315484	8000.190932	10.392051	-0.051349	4.815664
247.289843	7999.968440	10.397056	-0.051344	4.815599
247.387969	7999.864337	10.402061	-0.051362	4.815568
247.424888	7999.956760	10.407066	-0.051369	4.815595
247.434581	8000.013508	10.412071	-0.051371	4.815612
247.292231	8000.029349	10.417075	-0.051344	4.815617
247.396357	8000.171979	10.422080	-0.051364	4.815658
247.466657	8000.053543	10.427085	-0.051377	4.815623
247.514916	8000.192062	10.432090	-0.051386	4.815664
247.360701	7999.862848	10.437095	-0.051357	4.815568
247.406041	8000.019469	10.442099	-0.051366	4.815614
247.439995	7999.836383	10.447104	-0.051372	4.815560
247.421976	7999.958876	10.452109	-0.051369	4.815596
247.104356	8000.379727	10.457114	-0.051310	4.815720
247.455204	7999.979708	10.462119	-0.051375	4.815602
247.526265	8000.040656	10.467123	-0.051388	4.815619
247.485642	8000.094452	10.472128	-0.051381	4.815635
247.633148	8000.028519	10.477133	-0.051408	4.815615
247.393393	8000.328920	10.482138	-0.051364	4.815704
247.308760	8000.052083	10.487143	-0.051348	4.815624
247.452574	8000.098198	10.492147	-0.051375	4.815636
247.443727	8000.152510	10.497152	-0.051373	4.815652
247.411920	8000.037753	10.502157	-0.051367	4.815619
247.227045	8000.055039	10.507162	-0.051333	4.815625
247.319301	7999.883577	10.512167	-0.051350	4.815574
247.505865	7999.983769	10.517171	-0.051385	4.815603
247.352033	8000.023981	10.522176	-0.051356	4.815615
247.429961	7999.964392	10.527181	-0.051371	4.815597
247.399903	8000.135804	10.532186	-0.051365	4.815648
247.470705	8000.038730	10.537191	-0.051379	4.815619
247.463284	8000.097336	10.542195	-0.051377	4.815636
247.472490	8000.053713	10.547200	-0.051379	4.815623
247.571266	7999.868476	10.552205	-0.051397	4.815569
247.188580	8000.129184	10.557210	-0.051326	4.815647
247.515797	8000.170805	10.562215	-0.051387	4.815657
247.541852	8000.126388	10.567219	-0.051392	4.815644
247.256702	8000.072645	10.572224	-0.051339	4.815630
247.367571	8000.070178	10.577229	-0.051360	4.815629
247.264288	7999.957465	10.582234	-0.051340	4.815596
247.337952	7999.828408	10.587239	-0.051354	4.815558
247.102533	7999.937761	10.592243	-0.051310	4.815591
247.292756	7999.957937	10.597248	-0.051346	4.815596
247.499639	7999.881224	10.602253	-0.051384	4.815573
247.380235	8000.003139	10.607258	-0.051362	4.815609
247.362940	7999.911041	10.612263	-0.051359	4.815582
247.469311	7999.951208	10.617267	-0.051379	4.815593
247.148056	7999.981226	10.622272	-0.051319	4.815604
247.393167	7999.783420	10.627277	-0.051365	4.815545
247.426251	8000.050881	10.632282	-0.051371	4.815623
247.616944	7999.846851	10.637287	-0.051406	4.815562
247.460862	8000.245770	10.642291	-0.051378	4.815680
247.483645	8000.095598	10.647296	-0.051382	4.815636
247.485765	7999.853271	10.652301	-0.051382	4.815565
247.283942	8000.072073	10.657306	-0.051345	4.815630
247.481747	8000.111592	10.662311	-0.051382	4.815640
247.457624	8000.189145	10.667315	-0.051377	4.815663
247.491626	7999.984704	10.672320	-0.051383	4.815603
247.540974	7999.969493	10.677325	-0.051393	4.815598
247.277184	8000.138176	10.682330	-0.051344	4.815649
247.512400	7999.945546	10.687335	-0.051387	4.815592
247.411251	8000.106195	10.692339	-0.051369	4.815639
247.475961	8000.177717	10.697344	-0.051381	4.815660
247.448678	8000.027800	10.702349	-0.051376	4.815616
247.426157	8000.126732	10.707354	-0.051372	4.815645
247.404282	7999.951280	10.712359	-0.051367	4.815594
247.514294	8000.096140	10.717363	-0.051388	4.815636
247.519216	8000.191248	10.722368	-0.051389	4.815663
247.670532	8000.047436	10.727373	-0.051417	4.815621
247.643994	8000.021383	10.732378	-0.051412	4.815613
247.556058	7999.842722	10.737383	-0.051396	4.815561
247.345485	8000.038961	10.742387	-0.051357	4.815620
247.487606	7999.969738	10.747392	-0.051383	4.815599
247.462554	7999.938372	10.752397	-0.051379	4.815590
247.448925	7999.996876	10.757402	-0.051376	4.815607
247.435534	8000.024421	10.762407	-0.051374	4.815615
247.666909	8000.068756	10.767411	-0.051417	4.815627
247.398624	8000.166898	10.772416	-0.051367	4.815657
247.693045	7999.952809	10.777421	-0.051422	4.815593
247.452050	8000.075951	10.782426	-0.051377	4.815630
247.653705	7999.943634	10.787431	-0.051414	4.815590
247.548892	8000.110630	10.792435	-0.051395	4.815640
247.511897	7999.980841	10.797440	-0.051388	4.815602
247.654719	8000.078189	10.802445	-0.051415	4.815630
247.736038	8000.082717	10.807450	-0.051430	4.815631
247.790983	7999.980046	10.812455	-0.051440	4.815600
247.741117	8000.137258	10.817459	-0.051431	4.815646
247.734957	8000.179870	10.822464	-0.051430	4.815659
247.533311	7999.958787	10.827469	-0.051392	4.815595
247.758516	8000.276352	10.832474	-0.051434	4.815687
247.710634	7999.993705	10.837479	-0.051425	4.815605
247.493990	8000.053182	10.842483	-0.051385	4.815623
247.457689	8000.099573	10.847488	-0.051378	4.815637
247.606344	7999.967463	10.852493	-0.051406	4.815597
247.612111	8000.082870	10.857498	-0.051407	4.815631
247.560135	7999.817243	10.862503	-0.051397	4.815554
247.747773	8000.074404	10.867507	-0.051433	4.815628
247.569268	8000.045882	10.872512	-0.051399	4.815621
247.649407	7999.975652	10.877517	-0.051414	4.815600
247.636036	8000.139863	10.882522	-0.051412	4.815648
247.654336	8000.005634	10.887527	-0.051415	4.815608
247.736931	8000.019791	10.892531	-0.051431	4.815612
247.580252	8000.154981	10.897536	-0.051402	4.815652
247.715377	7999.846482	10.902541	-0.051427	4.815562
247.554013	8000.047792	10.907546	-0.051397	4.815621
247.664043	7999.963100	10.912551	-0.051417	4.815596
247.822221	8000.149317	10.917555	-0.051447	4.815650
247.708339	8000.130386	10.922560	-0.051426	4.815645
247.646204	8000.162478	10.927565	-0.051414	4.815654
247.630243	8000.153680	10.932570	-0.051411	4.815652
247.881390	7999.848133	10.937575	-0.051458	4.815561
247.575939	7999.995853	10.942579	-0.051401	4.815606
247.536109	8000.062474	10.947584	-0.051394	4.815626
247.849577	8000.072909	10.952589	-0.051452	4.815627
247.651237	8000.097449	10.957594	-0.051415	4.815635
247.863868	7999.980258	10.962599	-0.051455	4.815600
247.986713	7999.999340	10.967603	-0.051478	4.815605
247.847825	8000.088909	10.972608	-0.051452	4.815632
247.896019	8000.013888	10.977613	-0.051461	4.815610
247.937217	8000.208883	10.982618	-0.051469	4.815666
247.794132	8000.022916	10.987623	-0.051442	4.815613
247.683540	7999.992295	10.992627	-0.051421	4.815604
247.552590	8000.059570	10.997632	-0.051397	4.815625
247.723464	8000.061282	11.002637	-0.051429	4.815624
247.574045	7999.963833	11.007642	-0.051401	4.815596
247.589392	7999.947003	11.012647	-0.051404	4.815592
247.621989	8000.031883	11.017651	-0.051410	4.815616
247.897969	8000.123922	11.022656	-0.051462	4.815642
247.953303	7999.970007	11.027661	-0.051472	4.815596
247.714456	7999.973604	11.032666	-0.051428	4.815599
247.682301	7999.995506	11.037671	-0.051422	4.815605
247.714014	8000.040868	11.042675	-0.051428	4.815618
247.830156	8000.103617	11.047680	-0.051449	4.815636
248.032021	8000.060989	11.052685	-0.051487	4.815623
247.927620	8000.140441	11.057690	-0.051467	4.815646
247.705384	8000.016183	11.062695	-0.051426	4.815611
247.601274	8000.079624	11.067699	-0.051407	4.815630
247.783091	7999.941646	11.072704	-0.051441	4.815589
247.812828	7999.997652	11.077709	-0.051446	4.815605
247.661706	8000.101969	11.082714	-0.051418	4.815636
247.859384	8000.035784	11.087719	-0.051455	4.815616
247.692959	8000.066182	11.092723	-0.051424	4.815626
247.826732	8000.151639	11.097728	-0.051449	4.815650
247.867601	7999.976136	11.102733	-0.051457	4.815599
247.761105	8000.242402	11.107738	-0.051437	4.815677
247.772222	7999.952171	11.112743	-0.051439	4.815592
247.620187	7999.980668	11.117747	-0.051411	4.815601
247.817641	8000.157914	11.122752	-0.051447	4.815652
247.919564	7999.986606	11.127757	-0.051466	4.815601
247.675647	8000.218607	11.132762	-0.051421	4.815670
247.877729	8000.218691	11.137767	-0.051459	4.815670
248.200724	8000.044569	11.142771	-0.051519	4.815617
247.895389	8000.159193	11.147776	-0.051462	4.815652
247.982228	8000.143524	11.152781	-0.051478	4.815647
247.818834	8000.138737	11.157786	-0.051448	4.815646
247.834979	8000.066398	11.162791	-0.051451	4.815625
247.790141	8000.156427	11.167795	-0.051443	4.815652
247.861648	8000.314546	11.172800	-0.051456	4.815698
247.978785	8000.197937	11.177805	-0.051478	4.815663
247.864596	8000.049809	11.182810	-0.051457	4.815620
247.975895	8000.066569	11.187815	-0.051477	4.815625
247.841097	8000.065449	11.192819	-0.051452	4.815625
247.777738	8000.050543	11.197824	-0.051441	4.815621
247.806000	7999.989079	11.202829	-0.051446	4.815603
247.910178	8000.146659	11.207834	-0.051465	4.815648
247.762514	8000.146398	11.212839	-0.051438	4.815649
247.869258	8000.034959	11.217843	-0.051458	4.815616
247.919616	8000.127603	11.222848	-0.051467	4.815643
248.025847	7999.863476	11.227853	-0.051487	4.815565
247.837751	8000.187138	11.232858	-0.051452	4.815660
247.850953	7999.862776	11.237863	-0.051454	4.815566
247.960452	7999.854949	11.242867	-0.051475	4.815563
247.905053	7999.975769	11.247872	-0.051465	4.815598
247.948814	8000.044816	11.252877	-0.051473	4.815618
247.804735	8000.030733	11.257882	-0.051446	4.815615
247.735231	8000.027471	11.262887	-0.051433	4.815614
247.761189	8000.137869	11.267891	-0.051438	4.815646
247.919736	8000.210918	11.272896	-0.051468	4.815667
248.106121	7999.882962	11.277901	-0.051502	4.815570
247.768710	8000.052585	11.282906	-0.051439	4.815621
247.975212	7999.980137	11.287911	-0.051478	4.815599
248.084315	8000.130324	11.292915	-0.051498	4.815643
248.117996	8000.114859	11.297920	-0.051505	4.815638
248.069091	8000.124744	11.302925	-0.051496	4.815641
248.063979	8000.152425	11.307930	-0.051495	4.815649
248.070891	8000.157879	11.312935	-0.051496	4.815651
248.027292	8000.193476	11.317939	-0.051488	4.815661
247.922407	8000.246227	11.322944	-0.051469	4.815677
248.080197	7999.951973	11.327949	-0.051498	4.815591
248.019323	7999.983018	11.332954	-0.051486	4.815600
247.868115	8000.007256	11.337959	-0.051458	4.815608
248.150891	8000.021464	11.342963	-0.051511	4.815611
247.997180	8000.147094	11.347968	-0.051483	4.815648
247.982197	7999.828680	11.352973	-0.051480	4.815555
248.161433	7999.956515	11.357978	-0.051513	4.815592
248.132699	8000.026519	11.362983	-0.051508	4.815612
247.990338	7999.985772	11.367987	-0.051481	4.815601
248.154069	8000.127238	11.372992	-0.051512	4.815641
248.105042	7999.932122	11.377997	-0.051503	4.815585
248.052716	8000.110649	11.383002	-0.051493	4.815637
247.974892	7999.954571	11.388007	-0.051479	4.815592
248.139872	7999.941239	11.393011	-0.051509	4.815587
248.074217	8000.178273	11.398016	-0.051497	4.815657
247.842594	7999.958837	11.403021	-0.051454	4.815594
248.028544	8000.099595	11.408026	-0.051489	4.815634
248.061223	8000.101197	11.413031	-0.051495	4.815634
247.847284	8000.106265	11.418035	-0.051455	4.815637
247.921429	8000.146978	11.423040	-0.051469	4.815648
248.108335	7999.962103	11.428045	-0.051504	4.815593
247.907289	7999.981261	11.433050	-0.051466	4.815600
247.799331	7999.849252	11.438055	-0.051446	4.815562
248.225498	7999.996047	11.443059	-0.051526	4.815603
248.085566	8000.062109	11.448064	-0.051500	4.815623
247.975886	7999.875619	11.453069	-0.051479	4.815569
247.933864	8000.104494	11.458074	-0.051472	4.815636
248.043489	7999.940785	11.463079	-0.051492	4.815587
248.004673	8000.002084	11.468083	-0.051485	4.815606
248.061225	7999.979516	11.473088	-0.051495	4.815599
248.111571	7999.925885	11.478093	-0.051505	4.815583
247.992325	8000.219705	11.483098	-0.051483	4.815669
248.101418	7999.968434	11.488103	-0.051503	4.815595
248.030320	7999.949131	11.493107	-0.051490	4.815590
248.089488	8000.174314	11.498112	-0.051501	4.815656
248.070367	8000.035204	11.503117	-0.051497	4.815615
248.046247	7999.969686	11.508122	-0.051493	4.815596
248.005051	7999.992509	11.513127	-0.051485	4.815603
248.114213	7999.946240	11.518131	-0.051505	4.815589
248.121026	8000.264531	11.523136	-0.051507	4.815682
248.301303	8000.034702	11.528141	-0.051540	4.815614
248.249355	8000.112872	11.533146	-0.051531	4.815637
248.172869	8000.345462	11.538151	-0.051517	4.815705
248.097873	8000.002578	11.543155	-0.051503	4.815605
248.065772	8000.121642	11.548160	-0.051497	4.815640
248.142292	7999.977681	11.553165	-0.051511	4.815598
248.273617	8000.170939	11.558170	-0.051536	4.815654
248.234310	8000.065667	11.563175	-0.051528	4.815623
248.195976	7999.951871	11.568179	-0.051521	4.815590
247.903452	8000.133968	11.573184	-0.051467	4.815645
248.041186	7999.858608	11.578189	-0.051492	4.815563
248.225927	8000.142419	11.583194	-0.051527	4.815646
248.018489	8000.079259	11.588199	-0.051488	4.815628
248.328350	8000.147293	11.593203	-0.051546	4.815646
248.312845	8000.277306	11.598208	-0.051543	4.815685
248.348887	8000.029117	11.603213	-0.051550	4.815612
248.244628	8000.112843	11.608218	-0.051530	4.815637
248.208129	8000.260665	11.613223	-0.051524	4.815680
248.117718	7999.958104	11.618227	-0.051507	4.815592
247.987456	7999.978413	11.623232	-0.051483	4.815599
248.223752	8000.128532	11.628237	-0.051527	4.815641
248.184200	8000.273101	11.633242	-0.051520	4.815684
248.172493	8000.231273	11.638247	-0.051517	4.815672
248.101099	8000.243996	11.643251	-0.051504	4.815676
248.013890	8000.202008	11.648256	-0.051488	4.815664
248.171395	7999.996368	11.653261	-0.051517	4.815603
248.073488	8000.331110	11.658266	-0.051499	4.815701
248.068532	8000.171942	11.663271	-0.051498	4.815655
248.187917	7999.959277	11.668275	-0.051520	4.815592
248.079145	8000.112329	11.673280	-0.051500	4.815637
248.247440	7999.967724	11.678285	-0.051531	4.815594
248.231491	8000.067833	11.683290	-0.051529	4.815624
248.248477	7999.972018	11.688295	-0.051532	4.815596
248.318598	7999.934724	11.693299	-0.051545	4.815584
248.156752	8000.258816	11.698304	-0.051515	4.815680
248.160320	7999.879841	11.703309	-0.051515	4.815569
248.123006	8000.163247	11.708314	-0.051509	4.815652
248.133517	7999.941338	11.713319	-0.051510	4.815587
248.230963	8000.068914	11.718323	-0.051529	4.815624
248.169112	8000.079657	11.723328	-0.051517	4.815627
248.237246	8000.071158	11.728333	-0.051530	4.815625
248.250299	7999.946451	11.733338	-0.051532	4.815588
248.196117	8000.026720	11.738343	-0.051522	4.815612
248.173284	8000.102159	11.743347	-0.051518	4.815634
248.285298	8000.079425	11.748352	-0.051539	4.815627
248.300342	7999.984647	11.753357	-0.051542	4.815599
248.129726	8000.112138	11.758362	-0.051510	4.815637
247.990165	8000.139768	11.763367	-0.051484	4.815646
248.188631	7999.915576	11.768371	-0.051521	4.815579
248.089667	8000.073059	11.773376	-0.051503	4.815626
248.240118	7999.839545	11.778381	-0.051531	4.815557
248.139995	8000.133675	11.783386	-0.051512	4.815643
248.160787	7999.961047	11.788391	-0.051516	4.815593
248.169600	7999.872575	11.793395	-0.051518	4.815567
248.145720	7999.962944	11.798400	-0.051513	4.815593
248.287677	7999.963119	11.803405	-0.051540	4.815593
248.278695	8000.003549	11.808410	-0.051538	4.815605
248.292988	7999.996310	11.813415	-0.051541	4.815602
248.419196	7999.944979	11.818419	-0.051564	4.815587
248.337373	8000.115554	11.823424	-0.051549	4.815637
248.242505	7999.828938	11.828429	-0.051531	4.815554
248.192403	8000.008568	11.833434	-0.051522	4.815606
248.159368	7999.989884	11.838439	-0.051516	4.815601
248.265907	8000.019379	11.843443	-0.051536	4.815609
248.328747	8000.176289	11.848448	-0.051548	4.815655
248.235002	7999.950550	11.853453	-0.051530	4.815589
248.192365	8000.003245	11.858458	-0.051522	4.815605
248.259679	7999.862338	11.863463	-0.051535	4.815563
248.470807	7999.875381	11.868467	-0.051574	4.815566
248.199666	7999.995899	11.873472	-0.051524	4.815603
248.203195	8000.009840	11.878477	-0.051525	4.815607
248.174892	8000.136440	11.883482	-0.051520	4.815644
248.320075	8000.113178	11.888487	-0.051547	4.815636
248.235548	8000.015714	11.893491	-0.051531	4.815608
248.075081	7999.968266	11.898496	-0.051501	4.815595
248.278421	7999.938474	11.903501	-0.051539	4.815586
248.203599	8000.009866	11.908506	-0.051525	4.815607
248.304584	7999.957057	11.913511	-0.051544	4.815591
248.333250	7999.907344	11.918515	-0.051549	4.815576
248.103931	7999.965547	11.923520	-0.051506	4.815594
248.405744	7999.862617	11.928525	-0.051563	4.815563
248.346020	8000.111493	11.933530	-0.051552	4.815636
248.600582	8000.087874	11.938535	-0.051599	4.815628
248.524415	7999.832524	11.943539	-0.051585	4.815553
248.356345	8000.145837	11.948544	-0.051554	4.815646
248.528922	7999.945780	11.953549	-0.051586	4.815587
248.329066	8000.051441	11.958554	-0.051549	4.815618
248.230671	7999.986851	11.963559	-0.051530	4.815600
248.407327	7999.901105	11.968563	-0.051563	4.815574
248.379087	8000.039451	11.973568	-0.051558	4.815615
248.462105	7999.985283	11.978573	-0.051574	4.815598
248.331794	7999.974627	11.983578	-0.051549	4.815596
248.298052	7999.955930	11.988583	-0.051543	4.815591
248.259292	7999.993741	11.993587	-0.051536	4.815602
248.323377	7999.981973	11.998592	-0.051548	4.815598
248.438584	8000.050047	12.003597	-0.051569	4.815617
248.300757	7999.911144	12.008602	-0.051544	4.815577
248.269389	8000.052642	12.013607	-0.051538	4.815619
248.328755	8000.056813	12.018611	-0.051549	4.815620
248.292264	8000.239870	12.023616	-0.051542	4.815674
248.365834	7999.988021	12.028621	-0.051556	4.815600
248.233492	8000.056342	12.033626	-0.051531	4.815620
248.386444	8000.006513	12.038631	-0.051560	4.815605
248.338821	7999.919258	12.043635	-0.051551	4.815580
248.118514	8000.074769	12.048640	-0.051510	4.815626
248.441090	7999.915588	12.053645	-0.051570	4.815578
248.548553	7999.928014	12.058650	-0.051590	4.815581
248.483394	7999.978209	12.063655	-0.051578	4.815596
248.402734	7999.943802	12.068659	-0.051563	4.815587
248.328287	8000.072856	12.073664	-0.051549	4.815625
248.329038	7999.974642	12.078669	-0.051550	4.815596
248.248836	8000.303266	12.083674	-0.051535	4.815692
248.413764	8000.200245	12.088679	-0.051566	4.815661
248.527180	7999.963991	12.093683	-0.051587	4.815592
248.237349	7999.990248	12.098688	-0.051533	4.815601
248.437436	7999.931576	12.103693	-0.051570	4.815583
248.587320	8000.077088	12.108698	-0.051598	4.815625
248.274994	7999.988734	12.113703	-0.051540	4.815600
248.508823	7999.990402	12.118707	-0.051583	4.815600
248.475167	7999.969571	12.123712	-0.051577	4.815594
248.490926	7999.932461	12.128717	-0.051580	4.815583
248.464850	8000.088994	12.133722	-0.051575	4.815629
248.322832	7999.875283	12.138727	-0.051549	4.815567
248.498545	7999.864261	12.143731	-0.051581	4.815563
248.375735	7999.993596	12.148736	-0.051559	4.815601
248.529498	7999.854093	12.153741	-0.051587	4.815560
248.324546	8000.001312	12.158746	-0.051549	4.815604
248.257105	8000.089907	12.163751	-0.051537	4.815630
248.333666	7999.949149	12.168755	-0.051551	4.815588
248.169682	8000.068206	12.173760	-0.051521	4.815624
248.227131	7999.998674	12.178765	-0.051531	4.815603
248.349583	8000.092490	12.183770	-0.051554	4.815630
248.360145	8000.327564	12.188775	-0.051556	4.815699
248.425677	7999.992301	12.193779	-0.051568	4.815601
248.452910	8000.000221	12.198784	-0.051573	4.815603
248.370218	7999.932682	12.203789	-0.051558	4.815583
248.341282	8000.045392	12.208794	-0.051553	4.815616
248.264416	7999.952323	12.213799	-0.051538	4.815590
248.314018	7999.879461	12.218803	-0.051548	4.815568
248.594097	8000.125319	12.223808	-0.051600	4.815639
248.519341	7999.960746	12.228813	-0.051586	4.815591
248.352771	8000.062678	12.233818	-0.051555	4.815621
248.409285	8000.103105	12.238823	-0.051566	4.815633
248.154288	8000.049849	12.243827	-0.051518	4.815619
248.187962	7999.984202	12.248832	-0.051524	4.815599
248.280279	7999.847972	12.253837	-0.051542	4.815559
248.339680	8000.126544	12.258842	-0.051553	4.815640
248.178528	8000.080151	12.263847	-0.051523	4.815627
248.328830	8000.038821	12.268851	-0.051551	4.815615
248.225477	8000.237875	12.273856	-0.051532	4.815673
248.458055	7999.953376	12.278861	-0.051575	4.815589
248.455549	8000.224538	12.283866	-0.051575	4.815668
248.438108	8000.009646	12.288871	-0.051571	4.815606
248.442644	8000.012926	12.293875	-0.051572	4.815606
248.416215	7999.970859	12.298880	-0.051567	4.815594
248.653209	7999.869011	12.303885	-0.051611	4.815563
248.653752	7999.875429	12.308890	-0.051612	4.815565
248.475442	8000.023082	12.313895	-0.051579	4.815609
248.594251	7999.870198	12.318899	-0.051601	4.815564
248.575776	7999.988416	12.323904	-0.051597	4.815599
248.578178	7999.912651	12.328909	-0.051598	4.815577
248.560940	7999.983911	12.333914	-0.051595	4.815597
248.669773	7999.964328	12.338919	-0.051615	4.815591
248.694559	7999.967938	12.343923	-0.051619	4.815592
248.582000	8000.229838	12.348928	-0.051599	4.815669
248.504636	8000.039597	12.353933	-0.051584	4.815614
248.589724	8000.209683	12.358938	-0.051600	4.815663
248.592250	8000.188373	12.363943	-0.051601	4.815657
248.610123	8000.041321	12.368947	-0.051604	4.815614
248.645913	8000.261858	12.373952	-0.051611	4.815678
248.678059	8000.041364	12.378957	-0.051617	4.815614
248.816057	8000.184550	12.383962	-0.051643	4.815655
248.622585	8000.023385	12.388967	-0.051606	4.815609
248.672227	7999.901408	12.393971	-0.051616	4.815573
248.471025	7999.995303	12.398976	-0.051578	4.815601
248.691957	7999.871839	12.403981	-0.051619	4.815564
248.589401	8000.000436	12.408986	-0.051600	4.815602
248.364441	8000.003190	12.413991	-0.051559	4.815604
248.579318	7999.910591	12.418995	-0.051599	4.815576
248.400749	7999.960010	12.424000	-0.051565	4.815591
248.744650	7999.973076	12.429005	-0.051629	4.815593
248.614512	8000.100158	12.434010	-0.051605	4.815631
248.749676	7999.967826	12.439015	-0.051630	4.815592
248.655763	7999.864870	12.444019	-0.051613	4.815562
248.458345	8000.060259	12.449024	-0.051576	4.815620
248.530494	7999.877789	12.454029	-0.051590	4.815567
248.543458	8000.017872	12.459034	-0.051592	4.815607
248.397014	7999.990938	12.464039	-0.051565	4.815600
248.431758	7999.986167	12.469043	-0.051571	4.815599
248.470250	8000.130938	12.474048	-0.051579	4.815641
248.504286	7999.954253	12.479053	-0.051585	4.815589
248.643267	7999.928755	12.484058	-0.051611	4.815581
248.575773	7999.882817	12.489063	-0.051598	4.815568
248.573146	7999.926554	12.494067	-0.051598	4.815581
248.526789	8000.016559	12.499072	-0.051589	4.815607
248.468792	7999.921661	12.504077	-0.051579	4.815580
248.533491	7999.914174	12.509082	-0.051591	4.815577
248.645318	7999.922401	12.514087	-0.051612	4.815579
248.495621	7999.903956	12.519091	-0.051584	4.815574
248.491781	7999.807803	12.524096	-0.051583	4.815546
248.669965	7999.869426	12.529101	-0.051616	4.815563
248.577337	7999.923444	12.534106	-0.051599	4.815580
248.392967	7999.878811	12.539111	-0.051565	4.815567
248.422113	7999.879288	12.544115	-0.051570	4.815567
248.440484	7999.889199	12.549120	-0.051574	4.815570
248.490412	7999.962617	12.554125	-0.051583	4.815592
248.567307	7999.980953	12.559130	-0.051597	4.815596
248.695870	7999.953150	12.564135	-0.051621	4.815588
248.474577	7999.873750	12.569139	-0.051580	4.815566
248.378712	7999.961882	12.574144	-0.051562	4.815592
248.457949	7999.827575	12.579149	-0.051577	4.815552
248.359322	7999.948761	12.584154	-0.051559	4.815588
248.402532	7999.883269	12.589159	-0.051567	4.815569
248.726283	7999.829809	12.594163	-0.051627	4.815552
248.437482	7999.943634	12.599168	-0.051573	4.815586
248.385252	7999.780498	12.604173	-0.051564	4.815539
248.569608	8000.039747	12.609178	-0.051598	4.815614
248.605643	7999.965596	12.614183	-0.051605	4.815592
248.575779	7999.984332	12.619187	-0.051599	4.815597
248.630119	7999.964932	12.624192	-0.051610	4.815592
248.500653	7999.884888	12.629197	-0.051585	4.815569
248.530237	7999.954773	12.634202	-0.051591	4.815589
248.446535	8000.078338	12.639207	-0.051576	4.815626
248.611364	7999.831176	12.644211	-0.051606	4.815552
248.555544	8000.035273	12.649216	-0.051596	4.815612
248.365911	7999.862428	12.654221	-0.051560	4.815563
248.558806	7999.920019	12.659226	-0.051596	4.815579
248.274495	7999.873762	12.664231	-0.051544	4.815567
248.409144	7999.896239	12.669235	-0.051569	4.815572
248.552313	7999.886824	12.674240	-0.051595	4.815569
248.601320	7999.879082	12.679245	-0.051605	4.815567
248.686677	7999.957348	12.684250	-0.051620	4.815589
248.401584	7999.977275	12.689255	-0.051567	4.815596
248.434340	7999.806977	12.694259	-0.051573	4.815546
248.339276	7999.875904	12.699264	-0.051556	4.815567
248.389425	7999.998441	12.704269	-0.051565	4.815602
248.510738	7999.960910	12.709274	-0.051588	4.815591
248.591253	8000.030556	12.714279	-0.051603	4.815611
248.684232	7999.892199	12.719283	-0.051620	4.815570
248.292766	8000.116466	12.724288	-0.051548	4.815637
248.449131	7999.937500	12.729293	-0.051577	4.815584
248.400345	8000.032804	12.734298	-0.051568	4.815612
248.298806	8000.110167	12.739303	-0.051549	4.815636
248.534977	7999.936769	12.744307	-0.051593	4.815584
248.500971	8000.203149	12.749312	-0.051587	4.815662
248.326260	7999.996378	12.754317	-0.051554	4.815602
248.433731	8000.088883	12.759322	-0.051574	4.815629
248.571762	8000.110349	12.764327	-0.051600	4.815634
248.754151	8000.003342	12.769331	-0.051634	4.815602
248.597978	8000.188726	12.774336	-0.051605	4.815657
248.589355	8000.066868	12.779341	-0.051603	4.815621
248.771629	8000.202233	12.784346	-0.051637	4.815660
248.620558	7999.985168	12.789351	-0.051609	4.815597
248.631797	7999.944780	12.794355	-0.051611	4.815586
248.569786	8000.106068	12.799360	-0.051600	4.815633
248.567681	7999.880750	12.804365	-0.051599	4.815567
248.497340	8000.012006	12.809370	-0.051586	4.815606
248.628467	8000.142267	12.814375	-0.051611	4.815643
248.531231	8000.008292	12.819379	-0.051593	4.815605
248.504845	8000.358080	12.824384	-0.051588	4.815707
248.555492	7999.986271	12.829389	-0.051597	4.815598
248.616710	7999.962712	12.834394	-0.051609	4.815591
248.498293	7999.982144	12.839399	-0.051587	4.815597
248.546476	7999.940222	12.844403	-0.051596	4.815585
248.540138	8000.123769	12.849408	-0.051595	4.815638
248.577329	8000.041095	12.854413	-0.051601	4.815614
248.556540	8000.109094	12.859418	-0.051598	4.815634
248.463916	8000.049935	12.864423	-0.051580	4.815617
248.552932	7999.891228	12.869427	-0.051597	4.815570
248.461861	8000.039231	12.874432	-0.051580	4.815614
248.550447	7999.928564	12.879437	-0.051597	4.815581
248.619562	7999.976670	12.884442	-0.051609	4.815595
248.557831	8000.027988	12.889447	-0.051598	4.815610
248.664410	7999.858889	12.894451	-0.051618	4.815560
248.767282	8000.090123	12.899456	-0.051637	4.815627
248.680068	7999.854879	12.904461	-0.051621	4.815559
248.500882	7999.960877	12.909466	-0.051588	4.815591
248.611339	7999.986165	12.914471	-0.051608	4.815598
248.493565	7999.896701	12.919475	-0.051586	4.815572
248.448117	7999.876747	12.924480	-0.051578	4.815567
248.563728	7999.889306	12.929485	-0.051599	4.815570
248.618708	7999.986297	12.934490	-0.051610	4.815598
248.612802	8000.008626	12.939495	-0.051609	4.815604
248.530574	7999.928282	12.944499	-0.051593	4.815581
248.553364	7999.880609	12.949504	-0.051598	4.815567
248.509204	7999.844660	12.954509	-0.051589	4.815557
248.597559	8000.031881	12.959514	-0.051606	4.815611
248.502465	8000.161668	12.964519	-0.051588	4.815650
248.617026	7999.845354	12.969523	-0.051610	4.815557
248.410098	8000.018166	12.974528	-0.051571	4.815608
248.549065	7999.974516	12.979533	-0.051597	4.815595
248.672841	7999.944500	12.984538	-0.051620	4.815585
248.409165	7999.863343	12.989543	-0.051571	4.815563
248.648818	7999.870444	12.994547	-0.051616	4.815564
248.444442	7999.965355	12.999552	-0.051578	4.815592
248.564696	7999.938484	13.004557	-0.051600	4.815584
248.709894	8000.045483	13.009562	-0.051627	4.815615
248.563843	8000.011081	13.014567	-0.051600	4.815605
248.781134	7999.902506	13.019571	-0.051640	4.815572
248.680109	8000.095192	13.024576	-0.051622	4.815629
248.814033	7999.897708	13.029581	-0.051647	4.815571
248.820204	7999.905286	13.034586	-0.051648	4.815573
248.655547	8000.052093	13.039591	-0.051617	4.815617
248.581062	8000.027396	13.044595	-0.051603	4.815610
248.696874	7999.982302	13.049600	-0.051625	4.815596
248.929748	7999.897469	13.054605	-0.051668	4.815570
248.866210	8000.016024	13.059610	-0.051657	4.815605
248.574905	7999.962178	13.064615	-0.051602	4.815591
248.743590	7999.953178	13.069619	-0.051634	4.815587
248.680684	8000.025831	13.074624	-0.051622	4.815609
248.670698	7999.881530	13.079629	-0.051620	4.815567
248.587187	8000.010437	13.084634	-0.051605	4.815605
248.644996	7999.965468	13.089639	-0.051616	4.815592
248.799707	7999.951970	13.094643	-0.051644	4.815587
248.706102	8000.030531	13.099648	-0.051627	4.815610
248.700810	7999.967452	13.104653	-0.051626	4.815592
248.731613	7999.891081	13.109658	-0.051632	4.815569
248.611719	8000.078121	13.114663	-0.051610	4.815625
248.772529	7999.856518	13.119667	-0.051640	4.815559
248.813389	8000.110234	13.124672	-0.051647	4.815633
248.902618	7999.823404	13.129677	-0.051664	4.815549
248.854960	8000.068208	13.134682	-0.051655	4.815621
248.896183	8000.143622	13.139687	-0.051663	4.815642
248.726434	8000.038364	13.144691	-0.051631	4.815612
248.604283	8000.233910	13.149696	-0.051609	4.815670
248.751204	7999.960829	13.154701	-0.051636	4.815590
248.972429	7999.873672	13.159706	-0.051677	4.815563
248.812435	8000.162563	13.164711	-0.051648	4.815648
248.786559	8000.067118	13.169715	-0.051643	4.815621
248.568988	8000.174627	13.174720	-0.051602	4.815653
248.537101	7999.962704	13.179725	-0.051596	4.815591
248.751781	8000.046275	13.184730	-0.051636	4.815615
248.761312	7999.947135	13.189735	-0.051638	4.815586
248.890252	7999.826447	13.194739	-0.051662	4.815550
248.797516	7999.978694	13.199744	-0.051645	4.815595
248.980449	8000.068157	13.204749	-0.051679	4.815620
248.982360	7999.878136	13.209754	-0.051679	4.815564
248.783036	7999.951775	13.214759	-0.051642	4.815587
249.010941	7999.872201	13.219763	-0.051685	4.815562
248.689996	7999.955608	13.224768	-0.051625	4.815588
248.815229	7999.988610	13.229773	-0.051648	4.815597
248.789308	7999.950822	13.234778	-0.051644	4.815587
248.725928	8000.106750	13.239783	-0.051632	4.815632
248.695430	7999.939693	13.244787	-0.051626	4.815584
248.680210	7999.996038	13.249792	-0.051623	4.815600
248.745170	7999.981081	13.254797	-0.051636	4.815596
248.926381	7999.874055	13.259802	-0.051669	4.815563
248.831302	7999.962201	13.264807	-0.051652	4.815590
248.946039	7999.857297	13.269811	-0.051673	4.815558
248.793725	8000.070504	13.274816	-0.051645	4.815621
248.736776	8000.005518	13.279821	-0.051634	4.815603
248.729377	7999.908239	13.284826	-0.051633	4.815574
248.612498	7999.952254	13.289831	-0.051611	4.815588
248.670561	7999.857107	13.294835	-0.051622	4.815560
248.603882	7999.899802	13.299840	-0.051609	4.815572
248.846237	7999.973146	13.304845	-0.051655	4.815593
248.653530	8000.050096	13.309850	-0.051619	4.815616
248.657194	8000.077919	13.314855	-0.051620	4.815624
248.755566	7999.955666	13.319859	-0.051638	4.815588
248.781161	8000.109837	13.324864	-0.051643	4.815633
248.863194	7999.955286	13.329869	-0.051658	4.815587
248.843202	8000.117258	13.334874	-0.051654	4.815635
248.849440	7999.978559	13.339879	-0.051656	4.815594
248.599571	7999.972365	13.344883	-0.051609	4.815594
248.658080	7999.989335	13.349888	-0.051620	4.815598
248.771687	7999.855585	13.354893	-0.051641	4.815559
248.653655	7999.869686	13.359898	-0.051619	4.815563
248.632359	8000.180049	13.364903	-0.051615	4.815654
248.933867	7999.789897	13.369907	-0.051671	4.815539
248.785996	8000.148386	13.374912	-0.051644	4.815644
248.857272	7999.863398	13.379917	-0.051657	4.815561
248.764850	7999.985754	13.384922	-0.051640	4.815597
248.705361	8000.115052	13.389927	-0.051629	4.815635
248.847373	7999.852570	13.394931	-0.051655	4.815557
248.813333	7999.971604	13.399936	-0.051649	4.815592
248.836529	8000.122533	13.404941	-0.051654	4.815636
248.910710	8000.055408	13.409946	-0.051668	4.815616
248.556780	8000.049657	13.414951	-0.051602	4.815616
248.848361	7999.891039	13.419955	-0.051656	4.815569
248.651755	8000.131287	13.424960	-0.051619	4.815640
248.689275	7999.962132	13.429965	-0.051626	4.815590
248.777750	8000.107716	13.434970	-0.051643	4.815632
248.773535	7999.909054	13.439975	-0.051642	4.815574
249.056854	7999.917934	13.444979	-0.051695	4.815576
248.704810	8000.084117	13.449984	-0.051629	4.815626
248.715629	7999.998879	13.454989	-0.051631	4.815601
248.950106	8000.002693	13.459994	-0.051675	4.815601
248.979978	8000.139851	13.464999	-0.051681	4.815641
248.976841	7999.910242	13.470003	-0.051680	4.815574
248.900799	8000.038204	13.475008	-0.051666	4.815611
248.981886	7999.996816	13.480013	-0.051681	4.815599
248.680199	8000.019676	13.485018	-0.051625	4.815607
248.574937	8000.112995	13.490023	-0.051606	4.815635
248.739000	7999.965117	13.495027	-0.051636	4.815591
248.675098	7999.985436	13.500032	-0.051624	4.815597
248.697642	7999.888643	13.505037	-0.051628	4.815569
248.756571	8000.122367	13.510042	-0.051640	4.815637
248.923964	7999.966001	13.515047	-0.051671	4.815590
248.932452	8000.104946	13.520051	-0.051672	4.815631
248.882717	8000.351856	13.525056	-0.051663	4.815703
248.798519	8000.145484	13.530061	-0.051648	4.815643
248.938101	8000.285495	13.535066	-0.051674	4.815684
248.914055	8000.243465	13.540071	-0.051669	4.815671
248.978850	7999.961573	13.545075	-0.051681	4.815589
248.845797	8000.165485	13.550080	-0.051657	4.815649
248.797137	8000.007741	13.555085	-0.051647	4.815603
248.942186	8000.030389	13.560090	-0.051674	4.815609
248.895379	7999.986922	13.565095	-0.051666	4.815596
248.978030	7999.955169	13.570099	-0.051681	4.815587
248.676356	8000.176626	13.575104	-0.051625	4.815653
248.902246	8000.043633	13.580109	-0.051667	4.815613
248.939079	7999.936394	13.585114	-0.051674	4.815582
248.881344	7999.938662	13.590119	-0.051663	4.815582
248.940549	7999.921477	13.595123	-0.051674	4.815577
248.993280	8000.092105	13.600128	-0.051684	4.815627
248.719748	8000.080187	13.605133	-0.051633	4.815625
248.843060	7999.980761	13.610138	-0.051656	4.815595
248.938500	8000.247113	13.615143	-0.051674	4.815672
248.966402	7999.981705	13.620147	-0.051679	4.815595
248.883905	8000.172558	13.625152	-0.051664	4.815651
248.750439	8000.090312	13.630157	-0.051639	4.815627
249.145509	7999.997439	13.635162	-0.051713	4.815598
248.956848	8000.153467	13.640167	-0.051678	4.815645
249.050915	7999.861374	13.645171	-0.051695	4.815559
248.956795	8000.162014	13.650176	-0.051678	4.815647
248.912432	7999.996866	13.655181	-0.051670	4.815599
248.913670	7999.901862	13.660186	-0.051670	4.815572
248.794689	8000.097459	13.665191	-0.051648	4.815629
248.746767	8000.073194	13.670195	-0.051639	4.815622
248.786130	8000.111207	13.675200	-0.051646	4.815633
248.856297	8000.218057	13.680205	-0.051659	4.815664
248.902416	7999.867528	13.685210	-0.051668	4.815562
248.747752	8000.153302	13.690215	-0.051639	4.815646
248.956404	7999.915391	13.695219	-0.051678	4.815575
248.814227	8000.083919	13.700224	-0.051652	4.815625
248.646291	8000.157000	13.705229	-0.051620	4.815647
248.750846	8000.079692	13.710234	-0.051640	4.815624
248.825960	8000.232534	13.715239	-0.051654	4.815669
248.753102	7999.997520	13.720243	-0.051640	4.815600
248.636613	8000.281780	13.725248	-0.051619	4.815684
248.828276	8000.152501	13.730253	-0.051655	4.815645
248.970139	8000.074731	13.735258	-0.051681	4.815622
248.821967	8000.189775	13.740263	-0.051653	4.815656
248.862129	7999.909620	13.745267	-0.051661	4.815574
248.804829	8000.042156	13.750272	-0.051650	4.815613
248.748771	7999.947289	13.755277	-0.051640	4.815586
248.819271	7999.981537	13.760282	-0.051653	4.815595
248.845203	8000.241420	13.765287	-0.051658	4.815671
248.941599	7999.987803	13.770291	-0.051676	4.815596
248.877555	8000.056167	13.775296	-0.051664	4.815617
248.878498	7999.963294	13.780301	-0.051664	4.815590
248.886154	7999.845973	13.785306	-0.051666	4.815555
248.759152	7999.990189	13.790311	-0.051642	4.815598
248.704286	8000.101411	13.795315	-0.051632	4.815631
248.708944	8000.017140	13.800320	-0.051633	4.815606
248.573381	8000.347002	13.805325	-0.051608	4.815703
248.766716	8000.024491	13.810330	-0.051644	4.815608
248.758386	8000.178112	13.815335	-0.051642	4.815653
248.838540	7999.961602	13.820339	-0.051657	4.815589
248.821977	8000.169542	13.825344	-0.051654	4.815650
248.964950	7999.871839	13.830349	-0.051681	4.815562
248.960710	7999.882451	13.835354	-0.051680	4.815566
248.877827	8000.003894	13.840359	-0.051664	4.815601
249.031221	7999.947666	13.845363	-0.051693	4.815584
248.954976	7999.931482	13.850368	-0.051679	4.815580
248.949147	8000.111836	13.855373	-0.051678	4.815633
249.142007	8000.022082	13.860378	-0.051714	4.815606
249.050644	8000.066512	13.865383	-0.051697	4.815619
248.821492	7999.927189	13.870387	-0.051654	4.815579
248.911625	8000.040769	13.875392	-0.051671	4.815612
248.966372	8000.091845	13.880397	-0.051681	4.815627
249.110978	7999.971410	13.885402	-0.051708	4.815591
248.902927	7999.978709	13.890407	-0.051669	4.815594
248.885607	7999.931451	13.895411	-0.051666	4.815580
248.787385	8000.154079	13.900416	-0.051648	4.815646
248.710881	7999.949971	13.905421	-0.051634	4.815587
248.765696	7999.892141	13.910426	-0.051644	4.815569
248.802432	8000.014461	13.915431	-0.051651	4.815605
248.765491	8000.183632	13.920435	-0.051644	4.815655
248.829807	7999.978610	13.925440	-0.051656	4.815594
248.870045	7999.961116	13.930445	-0.051664	4.815589
248.996048	7999.983454	13.935450	-0.051687	4.815595
248.808760	8000.069034	13.940455	-0.051652	4.815621
248.856468	7999.990801	13.945459	-0.051661	4.815598
248.871060	8000.040157	13.950464	-0.051664	4.815612
248.791977	8000.318620	13.955469	-0.051650	4.815694
248.848504	8000.025916	13.960474	-0.051660	4.815608
248.861449	8000.119022	13.965479	-0.051662	4.815635
248.820361	7999.968875	13.970483	-0.051655	4.815592
248.889378	7999.962526	13.975488	-0.051668	4.815589
248.705327	8000.118628	13.980493	-0.051633	4.815636
248.692415	7999.867508	13.985498	-0.051631	4.815562
248.668876	8000.159683	13.990503	-0.051627	4.815648
248.766605	7999.989372	13.995507	-0.051645	4.815598
248.727635	8000.109394	14.000512	-0.051638	4.815633
248.949177	7999.953908	14.005517	-0.051679	4.815587
248.937898	8000.014588	14.010522	-0.051677	4.815604
248.992017	8000.095551	14.015527	-0.051687	4.815628
248.875598	7999.940976	14.020531	-0.051665	4.815583
248.944115	8000.159910	14.025536	-0.051678	4.815647
248.875646	7999.973015	14.030541	-0.051665	4.815592
249.176101	7999.876469	14.035546	-0.051721	4.815563
249.027880	8000.027815	14.040551	-0.051694	4.815608
248.916468	7999.909625	14.045555	-0.051673	4.815574
249.145646	8000.102342	14.050560	-0.051716	4.815629
248.966960	7999.878420	14.055565	-0.051683	4.815564
249.025525	7999.901798	14.060570	-0.051694	4.815571
248.961493	7999.922114	14.065575	-0.051682	4.815577
248.986047	7999.954548	14.070579	-0.051686	4.815587
249.066486	7999.993230	14.075584	-0.051701	4.815597
249.138610	8000.094772	14.080589	-0.051715	4.815627
249.116544	7999.958815	14.085594	-0.051711	4.815587
248.866862	7999.944082	14.090599	-0.051664	4.815584
249.050790	7999.884079	14.095603	-0.051698	4.815566
249.165659	7999.928659	14.100608	-0.051720	4.815578
248.968566	8000.001266	14.105613	-0.051683	4.815600
248.819637	8000.145127	14.110618	-0.051656	4.815643
248.940593	8000.292309	14.115623	-0.051678	4.815685
249.094424	8000.170956	14.120627	-0.051707	4.815649
248.750851	7999.967844	14.125632	-0.051643	4.815592
248.562200	7999.963713	14.130637	-0.051608	4.815591
248.909383	7999.967224	14.135642	-0.051672	4.815591
248.824585	8000.186868	14.140647	-0.051657	4.815655
248.916740	7999.849901	14.145651	-0.051674	4.815556
248.996588	7999.975057	14.150656	-0.051689	4.815592
248.889578	8000.073687	14.155661	-0.051669	4.815622
248.996674	7999.988945	14.160666	-0.051689	4.815596
249.048009	8000.086946	14.165671	-0.051699	4.815625
249.146823	8000.010612	14.170675	-0.051717	4.815602
249.159413	8000.093035	14.175680	-0.051719	4.815626
249.012216	8000.026581	14.180685	-0.051692	4.815607
249.271512	7999.997700	14.185690	-0.051740	4.815598
248.990027	7999.855391	14.190695	-0.051688	4.815557
248.900209	7999.952164	14.195699	-0.051671	4.815586
248.892455	8000.023579	14.200704	-0.051670	4.815607
248.780511	7999.840251	14.205709	-0.051649	4.815554
248.809119	7999.949626	14.210714	-0.051654	4.815586
248.832128	8000.056775	14.215719	-0.051659	4.815617
249.012402	7999.925175	14.220723	-0.051692	4.815578
248.936398	7999.930350	14.225728	-0.051678	4.815580
248.952263	8000.080092	14.230733	-0.051681	4.815623
248.822591	7999.991501	14.235738	-0.051657	4.815598
248.912017	8000.067699	14.240743	-0.051674	4.815620
248.752892	7999.883603	14.245747	-0.051644	4.815567
248.576420	8000.000322	14.250752	-0.051611	4.815602
248.832583	7999.863550	14.255757	-0.051659	4.815561
248.858244	7999.886393	14.260762	-0.051664	4.815567
248.784205	7999.958865	14.265767	-0.051650	4.815589
249.067894	7999.899416	14.270771	-0.051703	4.815570
249.097463	8000.048314	14.275776	-0.051709	4.815613
248.877436	8000.063959	14.280781	-0.051668	4.815619
249.104255	7999.875459	14.285786	-0.051710	4.815563
248.915587	7999.591589	14.290791	-0.051675	4.815481

248.849122	7996.324755	14.295795	-0.051660	4.814526
248.904256	7990.726578	14.300800	-0.051667	4.812888
248.912286	7983.945490	14.305805	-0.051664	4.810904
248.798665	7976.688693	14.310810	-0.051638	4.808780
248.543916	7969.049301	14.315815	-0.051586	4.806543
248.563502	7961.242011	14.320819	-0.051584	4.804256
248.715945	7953.365923	14.325824	-0.051607	4.801946
248.532362	7945.364049	14.330829	-0.051568	4.799600
248.556177	7937.478779	14.335834	-0.051567	4.797286
248.533164	7929.416963	14.340839	-0.051558	4.794919
248.569988	7921.415259	14.345843	-0.051560	4.792568
248.543831	7913.398529	14.350848	-0.051550	4.790212
248.609709	7905.389169	14.355853	-0.051557	4.787857
248.610152	7897.392382	14.360858	-0.051552	4.785505
248.283724	7889.401460	14.365863	-0.051486	4.783154
248.466056	7881.428829	14.370867	-0.051514	4.780806
248.310741	7873.434411	14.375872	-0.051480	4.778451
248.159106	7865.414399	14.380877	-0.051447	4.776088
248.206578	7857.424258	14.385882	-0.051451	4.773731
248.073044	7849.344793	14.390887	-0.051420	4.771348
248.006039	7841.344264	14.395891	-0.051403	4.768987
247.825339	7833.409752	14.400896	-0.051364	4.766644
247.989026	7825.344986	14.405901	-0.051389	4.764260
248.069029	7817.461636	14.410906	-0.051399	4.761929
247.735946	7809.373653	14.415911	-0.051332	4.759538
247.800507	7801.426261	14.420915	-0.051339	4.757186
247.776726	7793.374262	14.425920	-0.051329	4.754802
247.616892	7785.316386	14.430925	-0.051294	4.752416
247.620004	7777.305469	14.435930	-0.051289	4.750041
247.573812	7769.339090	14.440935	-0.051276	4.747679
247.419320	7761.334537	14.445939	-0.051242	4.745305
247.230973	7753.338966	14.450944	-0.051202	4.742932
247.192544	7745.355296	14.455949	-0.051189	4.740561
247.214982	7737.399356	14.460954	-0.051188	4.738197
247.080419	7729.321970	14.465959	-0.051158	4.735797
246.986521	7721.347770	14.470963	-0.051135	4.733425
246.907039	7713.304325	14.475968	-0.051115	4.731032
246.779610	7705.224715	14.480973	-0.051086	4.728627
246.891893	7697.325348	14.485978	-0.051102	4.726273
246.996630	7689.284243	14.490983	-0.051116	4.723876
247.092199	7681.354925	14.495987	-0.051129	4.721512
247.021091	7673.321445	14.500992	-0.051111	4.719115
246.946967	7665.371529	14.505997	-0.051092	4.716743
246.844495	7657.391979	14.511002	-0.051067	4.714360
246.637024	7649.284073	14.516007	-0.051024	4.711938
246.880859	7641.299735	14.521011	-0.051064	4.709550
246.935415	7633.351358	14.526016	-0.051069	4.707173
246.599264	7625.279014	14.531021	-0.051001	4.704758
246.597061	7617.357150	14.536026	-0.050995	4.702386
246.437613	7609.278803	14.541031	-0.050961	4.699967
246.415937	7601.344105	14.546035	-0.050951	4.697589
246.394208	7593.319761	14.551040	-0.050942	4.695183
246.251284	7585.288390	14.556045	-0.050910	4.692773
246.270921	7577.264265	14.561050	-0.050909	4.690365
246.212893	7569.236536	14.566055	-0.050893	4.687954
246.221107	7561.309944	14.571059	-0.050889	4.685572
246.236185	7553.315788	14.576064	-0.050887	4.683169
246.049494	7545.266569	14.581069	-0.050847	4.680748
246.194269	7537.253347	14.586074	-0.050869	4.678336
246.195827	7529.341991	14.591079	-0.050864	4.675954
246.043761	7521.257826	14.596083	-0.050830	4.673519
246.066422	7513.155941	14.601088	-0.050829	4.671077
245.816607	7505.207201	14.606093	-0.050778	4.668680
245.895504	7497.243299	14.611098	-0.050787	4.666277
245.865021	7489.190000	14.616103	-0.050776	4.663846
245.656805	7481.242568	14.621107	-0.050732	4.661446
245.777802	7473.248829	14.626112	-0.050750	4.659030
245.710262	7465.274058	14.631117	-0.050732	4.656619
245.740986	7457.233598	14.636122	-0.050732	4.654187
245.436548	7449.232453	14.641127	-0.050671	4.651765
245.555086	7441.185218	14.646131	-0.050687	4.649328
245.399808	7433.240366	14.651136	-0.050653	4.646921
245.276491	7425.183428	14.656141	-0.050625	4.644479
245.336144	7417.283477	14.661146	-0.050631	4.642083
245.244701	7409.221703	14.666151	-0.050609	4.639636
245.411738	7401.255142	14.671155	-0.050635	4.637217
245.311010	7393.196710	14.676160	-0.050611	4.634769
245.261311	7385.169353	14.681165	-0.050596	4.632330
245.180236	7377.177006	14.686170	-0.050576	4.629899
245.082511	7369.196060	14.691175	-0.050553	4.627471
245.199724	7361.175432	14.696179	-0.050569	4.625029
245.066685	7353.209066	14.701184	-0.050540	4.622603
244.958649	7345.165018	14.706189	-0.050514	4.620151
245.147980	7337.228739	14.711194	-0.050544	4.617731
244.885937	7329.203445	14.716199	-0.050490	4.615283
244.696928	7321.187621	14.721203	-0.050450	4.612836
244.602851	7313.159743	14.726208	-0.050427	4.610385
244.582788	7305.131032	14.731213	-0.050418	4.607931
244.520500	7297.197505	14.736218	-0.050402	4.605506
244.546677	7289.176272	14.741223	-0.050401	4.603052
244.499183	7281.155320	14.746227	-0.050387	4.600598
244.651802	7273.213834	14.751232	-0.050411	4.598166
244.306648	7265.176407	14.756237	-0.050341	4.595703
244.346596	7257.142765	14.761242	-0.050343	4.593241
244.246402	7249.096395	14.766247	-0.050319	4.590773
244.311293	7241.129313	14.771251	-0.050326	4.588328
244.466271	7233.127623	14.776256	-0.050350	4.585871
244.162788	7225.145543	14.781261	-0.050288	4.583419
244.140040	7217.157963	14.786266	-0.050279	4.580964
244.165598	7209.118724	14.791271	-0.050279	4.578491
244.136497	7201.134712	14.796275	-0.050268	4.576035
244.147668	7193.156902	14.801280	-0.050265	4.573579
243.920470	7185.078831	14.806285	-0.050217	4.571090
243.872122	7177.137264	14.811290	-0.050203	4.568642
243.782298	7169.129290	14.816295	-0.050181	4.566173
243.756050	7161.138583	14.821299	-0.050171	4.563707
243.744634	7153.169339	14.826304	-0.050164	4.561247
243.806297	7145.114146	14.831309	-0.050170	4.558759
243.699546	7137.204500	14.836314	-0.050145	4.556315
243.500271	7129.097714	14.841319	-0.050103	4.553808
243.786167	7121.064668	14.846323	-0.050151	4.551323
243.668004	7113.114646	14.851328	-0.050124	4.548862
243.426379	7105.094067	14.856333	-0.050074	4.546377
243.486715	7097.118584	14.861338	-0.050080	4.543906
243.450444	7089.162079	14.866343	-0.050068	4.541439
243.253019	7081.088141	14.871347	-0.050026	4.538934
243.240139	7073.170447	14.876352	-0.050018	4.536476
243.029429	7065.134704	14.881357	-0.049974	4.533980
243.262480	7057.139733	14.886362	-0.050012	4.531496
243.081331	7049.108699	14.891367	-0.049973	4.528999
242.917363	7041.124194	14.896371	-0.049937	4.526515
243.054722	7033.103883	14.901376	-0.049958	4.524019
242.734041	7025.110361	14.906381	-0.049893	4.521529
242.924581	7017.135550	14.911386	-0.049923	4.519044
243.038281	7009.160647	14.916391	-0.049939	4.516558
243.046093	7001.101890	14.921395	-0.049935	4.514044
242.787744	6993.016789	14.926400	-0.049882	4.511520
242.727213	6985.015632	14.931405	-0.049866	4.509021
242.632655	6977.035213	14.936410	-0.049843	4.506528
242.461127	6969.054936	14.941415	-0.049806	4.504032
242.550860	6961.093793	14.946419	-0.049817	4.501542
242.505275	6953.081419	14.951424	-0.049804	4.499034
242.340875	6945.070655	14.956429	-0.049768	4.496525
242.447420	6937.081788	14.961434	-0.049783	4.494022
242.456346	6929.011671	14.966439	-0.049779	4.491492
242.332349	6921.029006	14.971443	-0.049751	4.488988
242.285709	6913.070956	14.976448	-0.049737	4.486490
242.168451	6905.049513	14.981453	-0.049710	4.483970
242.212441	6897.088560	14.986458	-0.049713	4.481469
242.193926	6889.044353	14.991463	-0.049704	4.478940
242.149978	6881.080386	14.996467	-0.049691	4.476434
242.035051	6873.074088	15.001472	-0.049664	4.473914
241.941347	6865.014637	15.006477	-0.049642	4.471375
241.981110	6857.041485	15.011482	-0.049644	4.468863
242.026687	6849.016315	15.016487	-0.049647	4.466333
241.848434	6841.011187	15.021491	-0.049609	4.463807
241.801939	6833.041718	15.026496	-0.049595	4.461291
241.758138	6825.051043	15.031501	-0.049582	4.458767
241.890287	6817.074591	15.036506	-0.049601	4.456247
241.647262	6809.012564	15.041511	-0.049551	4.453697
241.570718	6800.967930	15.046515	-0.049531	4.451152
241.669262	6793.004544	15.051520	-0.049544	4.448632
241.590915	6785.003624	15.056525	-0.049525	4.446097
241.524552	6777.021918	15.061530	-0.049507	4.443567
241.433179	6769.037256	15.066535	-0.049485	4.441035
241.326299	6761.007236	15.071539	-0.049460	4.438487
241.255584	6753.041346	15.076544	-0.049442	4.435958
241.212789	6744.980398	15.081549	-0.049428	4.433397
241.213805	6736.969661	15.086554	-0.049423	4.430851
240.946958	6728.909519	15.091559	-0.049368	4.428287
240.993302	6720.934888	15.096563	-0.049372	4.425750
241.212791	6712.974984	15.101568	-0.049408	4.423216
240.976406	6704.984315	15.106573	-0.049358	4.420670
241.067372	6697.000200	15.111578	-0.049370	4.418125
240.935139	6688.990840	15.116583	-0.049340	4.415570
240.794019	6680.945237	15.121587	-0.049309	4.413002
240.652894	6672.991378	15.126592	-0.049277	4.410462
240.626963	6664.947507	15.131597	-0.049267	4.407892
240.744753	6656.979235	15.136602	-0.049284	4.405345
240.581896	6649.006489	15.141607	-0.049249	4.402794
240.382526	6640.994185	15.146611	-0.049206	4.400229
240.515265	6633.036601	15.151616	-0.049226	4.397681
240.495070	6625.000471	15.156621	-0.049217	4.395106
240.445188	6616.965683	15.161626	-0.049203	4.392530
240.359822	6608.934311	15.166631	-0.049181	4.389953
240.474711	6600.956675	15.171635	-0.049198	4.387393
240.239569	6592.985032	15.176640	-0.049149	4.384831
240.214426	6584.962895	15.181645	-0.049139	4.382253
240.503191	6576.978610	15.186650	-0.049187	4.379687
240.242618	6569.049742	15.191655	-0.049134	4.377135
240.301046	6561.013037	15.196659	-0.049140	4.374548
240.249070	6552.992834	15.201664	-0.049125	4.371964
240.075089	6544.949696	15.206669	-0.049087	4.369371
239.829513	6537.002785	15.211674	-0.049036	4.366806
239.804857	6528.983832	15.216679	-0.049026	4.364219
239.748214	6521.024410	15.221683	-0.049011	4.361648
239.822908	6512.981138	15.226688	-0.049019	4.359050
239.873612	6505.010701	15.231693	-0.049024	4.356474
239.829898	6496.980289	15.236698	-0.049010	4.353876
239.683936	6488.836236	15.241703	-0.048978	4.351239
239.526336	6480.873787	15.246707	-0.048943	4.348659
239.557769	6472.944964	15.251712	-0.048944	4.346090
239.380828	6464.961651	15.256717	-0.048906	4.343501
239.480802	6456.971563	15.261722	-0.048919	4.340909
239.544889	6448.964866	15.266727	-0.048926	4.338310
239.590033	6440.928765	15.271731	-0.048929	4.335700
239.487932	6432.955420	15.276736	-0.048905	4.333108
239.322348	6424.908630	15.281741	-0.048869	4.330490
239.419616	6416.965523	15.286746	-0.048882	4.327906
239.215446	6408.932235	15.291751	-0.048839	4.325289
238.957236	6400.972168	15.296755	-0.048786	4.322693
239.001174	6392.966111	15.301760	-0.048789	4.320084
239.041598	6384.961134	15.306765	-0.048791	4.317473
238.928316	6376.978876	15.311770	-0.048765	4.314867
238.817225	6368.939328	15.316775	-0.048739	4.312240
238.804737	6360.887139	15.321779	-0.048731	4.309608
238.775627	6352.928085	15.326784	-0.048721	4.307006
238.636001	6344.904952	15.331789	-0.048690	4.304379
238.646210	6336.969932	15.336794	-0.048686	4.301782
238.745738	6328.889877	15.341799	-0.048700	4.299135
238.484417	6320.950199	15.346803	-0.048646	4.296531
238.507926	6312.927565	15.351808	-0.048645	4.293900
238.318217	6304.864730	15.356813	-0.048605	4.291252
238.242868	6296.890583	15.361818	-0.048585	4.288632
238.219774	6288.926678	15.366823	-0.048576	4.286015
238.436571	6280.882787	15.371827	-0.048611	4.283372
238.072563	6272.940206	15.376832	-0.048538	4.280756
237.942470	6264.917925	15.381837	-0.048509	4.278114
238.094552	6256.957765	15.386842	-0.048532	4.275493
237.971426	6248.883694	15.391847	-0.048504	4.272830
238.118065	6240.869117	15.396851	-0.048526	4.270188
238.026731	6232.896023	15.401856	-0.048504	4.267556
237.919852	6224.850811	15.406861	-0.048479	4.264898
237.784583	6216.915323	15.411866	-0.048448	4.262275
237.705111	6208.869058	15.416871	-0.048428	4.259614
237.713646	6200.932996	15.421875	-0.048425	4.256988
237.689763	6192.910338	15.426880	-0.048415	4.254332
237.376798	6184.882811	15.431885	-0.048352	4.251670
237.537907	6176.850995	15.436890	-0.048376	4.249009
237.357318	6168.892085	15.441895	-0.048338	4.246367
237.211612	6160.884562	15.446899	-0.048305	4.243708
237.308249	6152.956987	15.451904	-0.048318	4.241076
237.325602	6144.926688	15.456909	-0.048316	4.238408
237.079660	6136.964419	15.461914	-0.048265	4.235758
236.977161	6128.925221	15.466919	-0.048241	4.233082
237.096527	6120.873419	15.471923	-0.048258	4.230403
237.124644	6112.926793	15.476928	-0.048258	4.227756
237.009367	6104.877976	15.481933	-0.048231	4.225071
237.091285	6096.926691	15.486938	-0.048242	4.222420
237.025208	6088.908143	15.491943	-0.048224	4.219743
236.829566	6080.961239	15.496947	-0.048182	4.217086
236.906992	6072.930817	15.501952	-0.048192	4.214403
236.752753	6064.906039	15.506957	-0.048158	4.211718
236.804827	6056.888492	15.511962	-0.048162	4.209036
236.667165	6048.910815	15.516967	-0.048131	4.206363
236.795740	6040.922520	15.521971	-0.048150	4.203688
236.708695	6032.981403	15.526976	-0.048129	4.201024
236.474102	6024.980249	15.531981	-0.048080	4.198338
236.401440	6016.941992	15.536986	-0.048061	4.195638
236.453833	6008.848276	15.541991	-0.048066	4.192920
236.296720	6000.813882	15.546995	-0.048031	4.190217
236.239935	5992.850161	15.552000	-0.048016	4.187538
236.127430	5984.862780	15.557005	-0.047990	4.184849
236.169637	5976.909811	15.562010	-0.047992	4.182171
236.120362	5968.918634	15.567015	-0.047978	4.179477
236.052059	5960.892546	15.572019	-0.047960	4.176769
236.183490	5952.881693	15.577024	-0.047979	4.174068
235.976250	5944.879931	15.582029	-0.047935	4.171363
236.222244	5936.877418	15.587034	-0.047976	4.168662
236.015491	5928.886108	15.592039	-0.047932	4.165958
235.911782	5920.923319	15.597043	-0.047908	4.163263
235.928991	5912.911812	15.602048	-0.047906	4.160551
235.900931	5904.892349	15.607053	-0.047896	4.157834
235.842403	5896.932601	15.612058	-0.047880	4.155135
235.637640	5888.896667	15.617063	-0.047836	4.152406
235.707875	5880.817853	15.622067	-0.047844	4.149665
235.661031	5872.888146	15.627072	-0.047830	4.146971
235.522827	5864.825445	15.632077	-0.047799	4.144229
235.536944	5856.904035	15.637082	-0.047797	4.141535
235.591362	5848.868038	15.642087	-0.047802	4.138801
235.546483	5840.893150	15.647091	-0.047788	4.136084
235.522852	5832.873303	15.652096	-0.047779	4.133351
235.508687	5824.851112	15.657101	-0.047771	4.130615
235.420154	5816.893676	15.662106	-0.047749	4.127899
235.322551	5808.877875	15.667111	-0.047726	4.125160
235.434396	5800.871573	15.672115	-0.047741	4.122426
235.493867	5792.896224	15.677120	-0.047747	4.119700
235.337541	5784.921429	15.682125	-0.047713	4.116969
235.159908	5776.919069	15.687130	-0.047675	4.114227
235.280694	5768.888084	15.692135	-0.047692	4.111477
235.134564	5760.837055	15.697139	-0.047660	4.108715
234.881399	5752.880195	15.702144	-0.047607	4.105982
234.729266	5744.874870	15.707149	-0.047574	4.103232
234.714769	5736.895118	15.712154	-0.047566	4.100491
234.666440	5728.895696	15.717159	-0.047552	4.097740
234.622518	5720.879726	15.722163	-0.047538	4.094982
234.632308	5712.906975	15.727168	-0.047535	4.092238
234.454126	5704.881726	15.732173	-0.047497	4.089471
234.416809	5696.917091	15.737178	-0.047485	4.086726
234.478003	5688.898727	15.742183	-0.047491	4.083961
234.303539	5680.941288	15.747187	-0.047453	4.081212
234.285739	5672.969458	15.752192	-0.047445	4.078458
234.428913	5664.919789	15.757197	-0.047466	4.075678
234.240791	5656.934987	15.762202	-0.047426	4.072914
234.209340	5648.896118	15.767207	-0.047415	4.070131
234.042421	5640.908852	15.772211	-0.047379	4.067363
234.252136	5632.919746	15.777216	-0.047413	4.064597
234.071372	5624.935903	15.782221	-0.047374	4.061825
233.999898	5616.909897	15.787226	-0.047355	4.059039
233.925995	5608.964130	15.792231	-0.047336	4.056279
234.041613	5600.905424	15.797235	-0.047353	4.053480
233.966598	5592.948200	15.802240	-0.047334	4.050711
233.869682	5584.922942	15.807245	-0.047310	4.047917
234.010646	5576.905734	15.812250	-0.047331	4.045127
233.745300	5568.963255	15.817255	-0.047277	4.042356
233.592946	5560.923956	15.822259	-0.047243	4.039550
233.626502	5552.972650	15.827264	-0.047244	4.036776
233.558513	5544.901599	15.832269	-0.047226	4.033956
233.548342	5536.793529	15.837274	-0.047219	4.031123
233.425000	5528.848713	15.842279	-0.047191	4.028343
233.302975	5520.841603	15.847283	-0.047163	4.025539
233.420669	5512.900891	15.852288	-0.047180	4.022760
233.329424	5504.887568	15.857293	-0.047158	4.019950
233.349660	5496.931909	15.862298	-0.047157	4.017161
233.292610	5488.901616	15.867303	-0.047141	4.014342
232.879508	5480.876032	15.872307	-0.047059	4.011517
232.949812	5472.904729	15.877312	-0.047067	4.008717
233.025917	5464.877475	15.882317	-0.047076	4.005895
233.028302	5456.924819	15.887322	-0.047071	4.003097
232.871420	5448.914079	15.892327	-0.047036	4.000273
232.858502	5440.939684	15.897331	-0.047029	3.997463
232.796221	5432.936891	15.902336	-0.047012	3.994640
232.773088	5424.864585	15.907341	-0.047003	3.991790
232.830095	5416.874768	15.912346	-0.047008	3.988970
232.793522	5408.877272	15.917351	-0.046996	3.986143
232.715093	5400.884778	15.922355	-0.046976	3.983315
232.748717	5392.943896	15.927360	-0.046977	3.980505
232.675088	5384.927301	15.932365	-0.046958	3.977665
232.450928	5376.924462	15.937370	-0.046912	3.974825
232.353232	5368.912647	15.942375	-0.046888	3.971981
232.576840	5360.861417	15.947379	-0.046925	3.969128
232.445963	5352.958493	15.952384	-0.046895	3.966318
232.156370	5344.930118	15.957389	-0.046836	3.963460
232.249762	5336.986594	15.962394	-0.046848	3.960636
232.225265	5328.974622	15.967399	-0.046838	3.957784
232.201319	5320.977177	15.972403	-0.046829	3.954935
232.080774	5312.936819	15.977408	-0.046801	3.952066
232.022408	5304.930806	15.982413	-0.046785	3.949209
231.868065	5296.958067	15.987418	-0.046751	3.946361
231.904174	5288.980882	15.992423	-0.046753	3.943512
231.876366	5280.956752	15.997427	-0.046742	3.940642
232.006783	5272.981207	16.002432	-0.046762	3.937791
231.690825	5264.985741	16.007437	-0.046698	3.934923
231.764726	5256.967117	16.012442	-0.046706	3.932052
231.741419	5248.944421	16.017447	-0.046697	3.929175
231.665004	5240.967703	16.022451	-0.046677	3.926311
231.783037	5232.982634	16.027456	-0.046694	3.923446
231.314503	5225.001085	16.032461	-0.046602	3.920569
231.388132	5217.015248	16.037466	-0.046610	3.917699
231.250865	5208.976680	16.042471	-0.046579	3.914804
231.247940	5200.946739	16.047475	-0.046574	3.911912
231.334822	5192.969193	16.052480	-0.046585	3.909038
231.067979	5184.982953	16.057485	-0.046530	3.906153
231.089135	5176.981684	16.062490	-0.046529	3.903265
231.326081	5168.974190	16.067495	-0.046567	3.900378
230.954786	5161.002716	16.072499	-0.046493	3.897489
231.067677	5152.997154	16.077504	-0.046509	3.894595
230.880491	5144.946980	16.082509	-0.046469	3.891678
230.838986	5136.958948	16.087514	-0.046456	3.888783
230.701483	5128.988025	16.092519	-0.046425	3.885890
230.771663	5120.962118	16.097523	-0.046433	3.882980
230.703309	5113.002922	16.102528	-0.046415	3.880088
230.436837	5105.030298	16.107533	-0.046361	3.877186
230.623922	5096.994639	16.112538	-0.046390	3.874268
230.666470	5088.719818	16.117543	-0.046393	3.871257
230.486806	5080.825976	16.122547	-0.046354	3.868379
230.412755	5072.877526	16.127552	-0.046335	3.865480
230.444726	5064.922422	16.132557	-0.046336	3.862579
230.313715	5056.945485	16.137562	-0.046306	3.859665
230.142179	5048.997374	16.142567	-0.046269	3.856758
230.058888	5040.964230	16.147571	-0.046249	3.853819
230.243878	5032.958176	16.152576	-0.046278	3.850894
230.178088	5024.955068	16.157581	-0.046261	3.847963
230.088591	5016.966233	16.162586	-0.046239	3.845034
230.192519	5009.021183	16.167591	-0.046253	3.842122
230.010870	5001.020815	16.172595	-0.046214	3.839183
229.827118	4993.097309	16.177600	-0.046175	3.836269
229.898676	4985.029570	16.182605	-0.046183	3.833305
229.955372	4976.979073	16.187610	-0.046188	3.830345
229.742924	4969.020518	16.192615	-0.046143	3.827411
229.744228	4960.994922	16.197619	-0.046138	3.824455
229.640545	4953.061990	16.202624	-0.046114	3.821528
229.616471	4945.056160	16.207629	-0.046104	3.818573
229.610346	4937.057195	16.212634	-0.046098	3.815620
229.629992	4929.068003	16.217639	-0.046096	3.812668
229.526992	4921.037292	16.222643	-0.046072	3.809696
229.183122	4913.112143	16.227648	-0.046003	3.806755
229.192653	4905.041108	16.232653	-0.045999	3.803766
229.061441	4897.106775	16.237658	-0.045970	3.800822
229.115628	4889.076854	16.242663	-0.045975	3.797844
229.234589	4881.058623	16.247667	-0.045992	3.794870
229.201657	4873.031303	16.252672	-0.045980	3.791886
228.988339	4865.037022	16.257677	-0.045936	3.788909
229.018930	4857.026987	16.262682	-0.045936	3.785928
229.009820	4849.080099	16.267687	-0.045929	3.782968
228.808778	4841.058898	16.272691	-0.045887	3.779974
228.828713	4833.114460	16.277696	-0.045885	3.777011
228.714470	4825.069861	16.282701	-0.045859	3.774005
228.755945	4817.056507	16.287706	-0.045861	3.771012
228.912034	4809.051696	16.292711	-0.045885	3.768022
228.713836	4801.048996	16.297715	-0.045843	3.765023
228.661876	4793.128786	16.302720	-0.045828	3.762056
228.646132	4785.063588	16.307725	-0.045820	3.759032
228.777737	4777.130566	16.312730	-0.045839	3.756060
228.652756	4769.092482	16.317735	-0.045811	3.753039
228.640668	4761.038134	16.322739	-0.045803	3.750013
228.696182	4753.085678	16.327744	-0.045809	3.747024
228.425030	4745.043047	16.332749	-0.045753	3.743991
228.272704	4737.123066	16.337754	-0.045719	3.741004
228.357062	4729.140777	16.342759	-0.045730	3.737997
228.241365	4721.099742	16.347763	-0.045703	3.734961
228.256298	4713.132253	16.352768	-0.045701	3.731953
228.111440	4705.092133	16.357773	-0.045669	3.728912
228.129686	4697.106022	16.362778	-0.045667	3.725892
228.092990	4689.151332	16.367783	-0.045655	3.722881
228.050190	4681.166416	16.372787	-0.045642	3.719855
227.979309	4673.180771	16.377792	-0.045623	3.716826
227.830471	4665.147474	16.382797	-0.045591	3.713775
227.926303	4657.068049	16.387802	-0.045603	3.710709
227.785087	4649.109999	16.392807	-0.045572	3.707682
227.532647	4641.080419	16.397811	-0.045520	3.704621
227.679138	4633.175859	16.402816	-0.045542	3.701616
227.646476	4625.138654	16.407821	-0.045530	3.698554
227.351948	4617.203066	16.412826	-0.045470	3.695521
227.341751	4609.207165	16.417831	-0.045463	3.692469
227.394915	4601.140161	16.422835	-0.045468	3.689390
227.404417	4593.227277	16.427840	-0.045465	3.686365
227.435633	4585.158739	16.432845	-0.045465	3.683279
227.500562	4577.188445	16.437850	-0.045472	3.680230
227.375588	4569.238231	16.442855	-0.045444	3.677180
227.232338	4561.225102	16.447859	-0.045412	3.674103
227.285919	4553.225861	16.452864	-0.045417	3.671034
227.183697	4545.197481	16.457869	-0.045392	3.667948
226.975630	4537.177379	16.462874	-0.045349	3.664859
227.210929	4529.221689	16.467879	-0.045387	3.661804
227.230221	4521.206183	16.472883	-0.045386	3.658717
227.057854	4513.278506	16.477888	-0.045348	3.655657
226.725921	4505.221222	16.482893	-0.045281	3.652540
226.968952	4497.174412	16.487898	-0.045321	3.649439
227.031822	4489.246049	16.492903	-0.045328	3.646377
226.727744	4481.224540	16.497907	-0.045266	3.643267
226.892035	4473.256666	16.502912	-0.045292	3.640187
226.769555	4465.275064	16.507917	-0.045264	3.637092
226.650890	4457.266249	16.512922	-0.045236	3.633983
226.605799	4449.239920	16.517927	-0.045223	3.630867
226.673737	4441.218234	16.522931	-0.045230	3.627753
226.453849	4433.259701	16.527936	-0.045184	3.624653
226.165174	4425.298476	16.532941	-0.045125	3.621548
226.239467	4417.302615	16.537946	-0.045134	3.618436
226.292828	4409.299071	16.542951	-0.045139	3.615318
226.081371	4401.281973	16.547955	-0.045094	3.612185
226.215370	4393.293751	16.552960	-0.045114	3.609070
226.208934	4385.293625	16.557965	-0.045108	3.605943
226.162112	4377.312906	16.562970	-0.045094	3.602821
226.144044	4369.357800	16.567975	-0.045085	3.599706
226.036894	4361.367401	16.572979	-0.045060	3.596573
225.995232	4353.379306	16.577984	-0.045047	3.593439
225.876071	4345.325080	16.582989	-0.045020	3.590275
225.954082	4337.344774	16.587994	-0.045029	3.587142
225.880376	4329.342734	16.592999	-0.045010	3.583994
225.771506	4321.357460	16.598003	-0.044985	3.580848
225.671205	4313.423794	16.603008	-0.044961	3.577721
225.648779	4305.381383	16.608013	-0.044951	3.574550
225.541647	4297.378438	16.613018	-0.044926	3.571389
225.415373	4289.372977	16.618023	-0.044898	3.568224
225.364732	4281.375420	16.623027	-0.044883	3.565061
225.380300	4273.436100	16.628032	-0.044881	3.561921
225.164286	4265.448438	16.633037	-0.044835	3.558752
225.213211	4257.432558	16.638042	-0.044839	3.555576
225.213785	4249.368423	16.643047	-0.044834	3.552378
225.212154	4241.290499	16.648051	-0.044829	3.549170
225.150118	4233.352408	16.653056	-0.044812	3.546014
225.124612	4225.366893	16.658061	-0.044802	3.542837
225.074123	4217.385735	16.663066	-0.044788	3.539658
224.981766	4209.435297	16.668071	-0.044765	3.536488
224.778046	4201.415959	16.673075	-0.044722	3.533283
224.838325	4193.389438	16.678080	-0.044728	3.530081
224.695734	4185.442623	16.683085	-0.044696	3.526901
224.590851	4177.418235	16.688090	-0.044672	3.523689
224.683188	4169.461763	16.693095	-0.044684	3.520507
224.363582	4161.475475	16.698099	-0.044619	3.517298
224.665559	4153.473772	16.703104	-0.044670	3.514098
224.522523	4145.444305	16.708109	-0.044638	3.510871
224.480770	4137.444765	16.713114	-0.044625	3.507656
224.415050	4129.459094	16.718119	-0.044608	3.504443
224.421295	4121.496133	16.723123	-0.044604	3.501238
224.416018	4113.524319	16.728128	-0.044598	3.498027
224.223076	4105.531905	16.733133	-0.044557	3.494798
224.169652	4097.536063	16.738138	-0.044542	3.491569
224.177642	4089.553647	16.743143	-0.044538	3.488345
224.048873	4081.519902	16.748147	-0.044509	3.485092
224.209859	4073.575758	16.753152	-0.044534	3.481882
224.140344	4065.596216	16.758157	-0.044515	3.478647
224.157116	4057.574975	16.763162	-0.044513	3.475396
224.061936	4049.555514	16.768167	-0.044490	3.472138
223.894885	4041.530908	16.773171	-0.044454	3.468872
223.826591	4033.562090	16.778176	-0.044436	3.465630
223.624963	4025.596087	16.783181	-0.044394	3.462381
223.747402	4017.557312	16.788186	-0.044411	3.459110
223.715312	4009.618851	16.793191	-0.044400	3.455872
223.418899	4001.622736	16.798195	-0.044340	3.452599
223.564343	3993.597926	16.803200	-0.044362	3.449325
223.543683	3985.612422	16.808205	-0.044353	3.446059
223.278733	3977.609333	16.813210	-0.044298	3.442774
223.178682	3969.679055	16.818215	-0.044274	3.439522
223.179497	3961.665933	16.823219	-0.044269	3.436235
223.521788	3953.635637	16.828224	-0.044328	3.432950
223.356633	3945.593655	16.833229	-0.044292	3.429640
223.233520	3937.620559	16.838234	-0.044264	3.426357
223.307110	3929.638232	16.843239	-0.044272	3.423073
223.204128	3921.662189	16.848243	-0.044248	3.419783
223.048004	3913.734578	16.853248	-0.044214	3.416508
222.956595	3905.708012	16.858253	-0.044192	3.413191
222.869265	3897.683672	16.863258	-0.044170	3.409871
222.751282	3889.719526	16.868263	-0.044143	3.406573
222.584234	3881.716757	16.873267	-0.044107	3.403253
222.828288	3873.737200	16.878272	-0.044147	3.399954
222.761496	3865.765752	16.883277	-0.044129	3.396644
222.582489	3857.751423	16.888282	-0.044091	3.393310
222.676321	3849.659793	16.893287	-0.044103	3.389949
222.546877	3841.691720	16.898291	-0.044074	3.386629
222.474225	3833.732717	16.903296	-0.044055	3.383311
222.439270	3825.752169	16.908301	-0.044043	3.379982
222.457396	3817.785463	16.913306	-0.044042	3.376658
222.371692	3809.805561	16.918311	-0.044021	3.373321
222.202257	3801.773588	16.923315	-0.043984	3.369956
222.206220	3793.804217	16.928320	-0.043979	3.366621
222.244243	3785.804082	16.933325	-0.043981	3.363270
222.065838	3777.827525	16.938330	-0.043943	3.359918
222.022653	3769.877845	16.943335	-0.043930	3.356578
221.863988	3761.830242	16.948339	-0.043895	3.353190
221.847499	3753.835666	16.953344	-0.043887	3.349826
221.717289	3745.854546	16.958349	-0.043857	3.346461
221.664384	3737.867403	16.963354	-0.043842	3.343092
221.820772	3729.874553	16.968359	-0.043866	3.339725
221.587016	3721.918569	16.973363	-0.043818	3.336355
221.651679	3713.912167	16.978368	-0.043824	3.332972
221.535621	3705.899482	16.983373	-0.043798	3.329577
221.449325	3697.909355	16.988378	-0.043776	3.326188
221.628136	3689.924676	16.993383	-0.043805	3.322808
221.372112	3681.931285	16.998387	-0.043752	3.319405
221.387025	3674.006693	17.003392	-0.043749	3.316037
221.408695	3665.933323	17.008397	-0.043748	3.312603
221.354084	3657.924916	17.013402	-0.043733	3.309191
221.242346	3649.980388	17.018407	-0.043707	3.305800
220.980551	3642.004079	17.023411	-0.043653	3.302386
221.138286	3634.015443	17.028416	-0.043677	3.298979
221.026115	3626.029981	17.033421	-0.043651	3.295560
220.899422	3618.016994	17.038426	-0.043622	3.292125
220.842592	3610.028721	17.043431	-0.043607	3.288699
220.798979	3602.036700	17.048435	-0.043593	3.285269
220.849409	3594.077252	17.053440	-0.043598	3.281853
220.551227	3586.085052	17.058445	-0.043537	3.278406
220.550492	3578.095441	17.063450	-0.043532	3.274967
220.463931	3570.083640	17.068455	-0.043510	3.271513
220.505519	3562.067946	17.073459	-0.043513	3.268057
220.761400	3554.077283	17.078464	-0.043555	3.264618
220.577073	3546.123655	17.083469	-0.043516	3.261173
220.305112	3538.132465	17.088474	-0.043460	3.257706
220.340106	3530.129635	17.093479	-0.043461	3.254241
220.244991	3522.121386	17.098483	-0.043438	3.250765
220.322794	3514.148212	17.103488	-0.043448	3.247308
220.300502	3506.127397	17.108493	-0.043438	3.243822
220.291771	3498.146962	17.113498	-0.043432	3.240351
220.230021	3490.209393	17.118503	-0.043415	3.236892
219.910514	3482.179767	17.123507	-0.043350	3.233379
219.897146	3474.131907	17.128512	-0.043343	3.229867
219.705680	3466.159457	17.133517	-0.043302	3.226377
219.719130	3458.166551	17.138522	-0.043299	3.222882
219.704409	3450.205626	17.143527	-0.043291	3.219396
219.610644	3442.223743	17.148531	-0.043269	3.215894
219.598515	3434.255713	17.153536	-0.043261	3.212398
219.568559	3426.239085	17.158541	-0.043250	3.208876
219.330702	3418.257334	17.163546	-0.043201	3.205356
219.537319	3410.307547	17.168551	-0.043234	3.201866
219.355564	3402.322502	17.173555	-0.043195	3.198339
219.181146	3394.344244	17.178560	-0.043158	3.194812
219.241968	3386.305110	17.183565	-0.043164	3.191265
219.209634	3378.309199	17.188570	-0.043153	3.187728
219.280304	3370.322891	17.193575	-0.043161	3.184196
219.117713	3362.379062	17.198579	-0.043125	3.180669
218.999695	3354.417334	17.203584	-0.043098	3.177132
218.850583	3346.387434	17.208589	-0.043065	3.173560
219.075806	3338.353672	17.213594	-0.043102	3.169998
218.936911	3330.406117	17.218599	-0.043071	3.166454
218.796838	3322.406023	17.223603	-0.043040	3.162883
219.012164	3314.437874	17.228608	-0.043074	3.159338
218.891127	3306.463092	17.233613	-0.043047	3.155771
218.797421	3298.441687	17.238618	-0.043024	3.152180
218.702651	3290.454670	17.243623	-0.043001	3.148601
218.570800	3282.448387	17.248627	-0.042972	3.145007
218.710266	3274.492171	17.253632	-0.042992	3.141444
218.576505	3266.492576	17.258637	-0.042962	3.137845
218.583069	3258.513390	17.263642	-0.042958	3.134257
218.498675	3250.533602	17.268647	-0.042937	3.130661
218.131735	3242.552884	17.273651	-0.042864	3.127047
218.166180	3234.564639	17.278656	-0.042865	3.123444
218.131562	3226.600047	17.283661	-0.042854	3.119844
217.971646	3218.651609	17.288666	-0.042819	3.116242
218.068228	3210.623494	17.293671	-0.042832	3.112611
218.001712	3202.592075	17.298675	-0.042814	3.108967
218.113102	3194.607311	17.303680	-0.042829	3.105348
217.847720	3186.664065	17.308685	-0.042775	3.101727
217.802108	3178.662900	17.313690	-0.042761	3.098085
217.910946	3170.670019	17.318695	-0.042776	3.094449
217.720240	3162.682458	17.323699	-0.042736	3.090798
217.599360	3154.722669	17.328704	-0.042708	3.087158
217.752562	3146.704327	17.333709	-0.042731	3.083500
217.734649	3138.731179	17.338714	-0.042723	3.079851
217.440481	3130.812574	17.343719	-0.042663	3.076209
217.400398	3122.728686	17.348723	-0.042650	3.072499
217.509639	3114.703220	17.353728	-0.042665	3.068818
217.351746	3106.741756	17.358733	-0.042631	3.065149
217.270559	3098.796288	17.363738	-0.042611	3.061488
217.200624	3090.824694	17.368743	-0.042592	3.057810
217.150824	3082.811305	17.373747	-0.042578	3.054109
217.027527	3074.834802	17.378752	-0.042550	3.050418
216.972686	3066.850845	17.383757	-0.042534	3.046722
216.921224	3058.885689	17.388762	-0.042520	3.043030
216.835028	3050.923056	17.393767	-0.042499	3.039333
216.716163	3042.948681	17.398771	-0.042471	3.035625
216.790668	3034.948590	17.403776	-0.042480	3.031909
216.674207	3026.931219	17.408781	-0.042453	3.028172
216.606445	3018.937477	17.413786	-0.042435	3.024444
216.879135	3010.957519	17.418791	-0.042481	3.020733
216.738232	3002.981087	17.423795	-0.042449	3.017000
216.483469	2995.027874	17.428800	-0.042397	3.013267
216.535880	2986.996424	17.433805	-0.042401	3.009508
216.474695	2979.032182	17.438810	-0.042385	3.005771
216.446384	2971.065774	17.443815	-0.042374	3.002029
216.105734	2963.103807	17.448819	-0.042306	2.998269
216.279381	2955.116150	17.453824	-0.042333	2.994518
216.024412	2947.094473	17.458829	-0.042280	2.990725
216.011169	2939.093140	17.463834	-0.042273	2.986949
216.049733	2931.118215	17.468839	-0.042275	2.983182
215.810469	2923.167784	17.473843	-0.042225	2.979409
216.074389	2915.178436	17.478848	-0.042269	2.975638
216.112568	2907.160073	17.483853	-0.042271	2.971837
215.964658	2899.190943	17.488858	-0.042238	2.968045
215.882075	2891.213909	17.493863	-0.042218	2.964248
215.594804	2883.274397	17.498867	-0.042159	2.960453
215.803396	2875.287866	17.503872	-0.042193	2.956656
215.684550	2867.293229	17.508877	-0.042165	2.952834
215.450385	2859.289490	17.513882	-0.042117	2.948997
215.479506	2851.317974	17.518887	-0.042117	2.945183
215.270658	2843.352640	17.523891	-0.042073	2.941355
215.482614	2835.348143	17.528896	-0.042107	2.937525
215.530167	2827.364733	17.533901	-0.042111	2.933692
215.359833	2819.342868	17.538906	-0.042074	2.929824
215.362085	2811.405443	17.543911	-0.042069	2.926001
215.178991	2803.439823	17.548915	-0.042030	2.922149
215.319397	2795.447389	17.553920	-0.042051	2.918296
215.303147	2787.478131	17.558925	-0.042043	2.914441
215.036915	2779.388454	17.563930	-0.041988	2.910509
215.170157	2771.429227	17.568935	-0.042008	2.906656
214.974749	2763.471159	17.573939	-0.041966	2.902782
214.860153	2755.523864	17.578944	-0.041940	2.898911
214.778061	2747.552242	17.583949	-0.041919	2.895026
214.680764	2739.550180	17.588954	-0.041896	2.891119
214.664708	2731.574236	17.593959	-0.041888	2.887224
214.589678	2723.606059	17.598963	-0.041869	2.883325
214.587994	2715.618211	17.603968	-0.041863	2.879415
214.484535	2707.677413	17.608973	-0.041839	2.875516
214.292556	2699.675360	17.613978	-0.041798	2.871578
214.277843	2691.697509	17.618983	-0.041790	2.867656
214.100427	2683.703860	17.623987	-0.041752	2.863712
214.074106	2675.741658	17.628992	-0.041742	2.859786
214.004899	2667.782598	17.633997	-0.041724	2.855853
214.128501	2659.748374	17.639002	-0.041741	2.851889
214.039590	2651.794051	17.644007	-0.041720	2.847948
214.034761	2643.802863	17.649011	-0.041714	2.843987
213.957870	2635.861162	17.654016	-0.041694	2.840041
213.903806	2627.890909	17.659021	-0.041679	2.836077
213.748235	2619.876320	17.664026	-0.041645	2.832079
213.782838	2611.876471	17.669031	-0.041646	2.828094
213.798106	2603.876962	17.674035	-0.041644	2.824102
213.815806	2595.915940	17.679040	-0.041642	2.820124
213.516530	2587.981923	17.684045	-0.041581	2.816135
213.445098	2579.981476	17.689050	-0.041563	2.812121
213.462487	2572.008374	17.694055	-0.041561	2.808120
213.313605	2564.017382	17.699059	-0.041528	2.804094
213.583765	2556.026750	17.704064	-0.041573	2.800088
213.542695	2548.082779	17.709069	-0.041560	2.796081
213.386517	2540.095576	17.714074	-0.041526	2.792039
213.286078	2532.119110	17.719079	-0.041502	2.788000
213.135298	2524.146551	17.724083	-0.041469	2.783955
213.073820	2516.194955	17.729088	-0.041452	2.779919
212.889118	2508.243504	17.734093	-0.041413	2.775871
213.143923	2500.178804	17.739098	-0.041455	2.771785
213.113134	2492.235223	17.744103	-0.041444	2.767737
212.666268	2484.275578	17.749107	-0.041356	2.763651
212.731275	2476.309402	17.754112	-0.041363	2.759586
212.885640	2468.325514	17.759117	-0.041386	2.755511
212.738882	2460.274329	17.764122	-0.041354	2.751378
212.569468	2452.322513	17.769127	-0.041317	2.747287
212.350195	2444.349060	17.774131	-0.041271	2.743177
212.533184	2436.368565	17.779136	-0.041300	2.739081
212.344632	2428.420338	17.784141	-0.041260	2.734973
212.248240	2420.425468	17.789146	-0.041236	2.730841
212.324468	2412.453001	17.794151	-0.041245	2.726724
212.056820	2404.505772	17.799155	-0.041190	2.722593
212.075005	2396.533644	17.804160	-0.041189	2.718460
212.157701	2388.539485	17.809165	-0.041199	2.714314
211.859692	2380.558076	17.814170	-0.041138	2.710144
211.926364	2372.595104	17.819175	-0.041146	2.706000
211.779816	2364.622056	17.824179	-0.041113	2.701832
211.900553	2356.657906	17.829184	-0.041130	2.697678
211.655329	2348.711289	17.834189	-0.041080	2.693504
211.561232	2340.704137	17.839194	-0.041057	2.689301
211.850759	2332.733908	17.844199	-0.041106	2.685135
211.677603	2324.758312	17.849203	-0.041068	2.680931
211.536041	2316.820520	17.854208	-0.041037	2.676742
211.588900	2308.818394	17.859213	-0.041041	2.672524
211.350989	2300.818169	17.864218	-0.040992	2.668283
211.419918	2292.842946	17.869223	-0.041000	2.664068
211.227433	2284.884532	17.874227	-0.040959	2.659838
211.316637	2276.925033	17.879232	-0.040970	2.655619
211.144768	2268.937322	17.884237	-0.040933	2.651361
211.057548	2260.967687	17.889242	-0.040912	2.647111
211.132712	2253.007337	17.894247	-0.040920	2.642870
211.007449	2245.030932	17.899251	-0.040892	2.638601
210.805063	2237.102075	17.904256	-0.040849	2.634345
210.997100	2229.081323	17.909261	-0.040880	2.630059
210.901565	2221.110803	17.914266	-0.040857	2.625774
210.637281	2213.182928	17.919271	-0.040802	2.621494
210.733018	2205.190811	17.924275	-0.040815	2.617196
210.658647	2197.210326	17.929280	-0.040796	2.612885
210.666192	2189.216413	17.934285	-0.040792	2.608566
210.434949	2181.268633	17.939290	-0.040744	2.604249
210.636368	2173.306966	17.944295	-0.040776	2.599946
210.343701	2165.370952	17.949299	-0.040717	2.595616
210.250563	2157.243333	17.954304	-0.040694	2.591189
210.046334	2149.275811	17.959309	-0.040651	2.586833
210.048704	2141.327333	17.964314	-0.040646	2.582495
210.044337	2133.398473	17.969319	-0.040640	2.578159
210.078326	2125.416891	17.974323	-0.040641	2.573791
210.155645	2117.424895	17.979328	-0.040651	2.569411
210.096783	2109.485518	17.984333	-0.040635	2.565044
209.882892	2101.565128	17.989338	-0.040590	2.560670
209.936214	2093.614095	17.994343	-0.040594	2.556289
209.934313	2085.620691	17.999347	-0.040589	2.551873
209.697661	2077.676291	18.004352	-0.040540	2.547461
209.692491	2069.703966	18.009357	-0.040534	2.543042
209.494010	2061.752148	18.014362	-0.040491	2.538612
209.465888	2053.784176	18.019367	-0.040481	2.534178
209.316364	2045.804528	18.024371	-0.040448	2.529721
209.406545	2037.831263	18.029376	-0.040460	2.525277
209.327137	2029.886458	18.034381	-0.040440	2.520829
209.030762	2021.954613	18.039386	-0.040379	2.516364
209.275216	2013.935533	18.044391	-0.040420	2.511882
209.100442	2005.935481	18.049395	-0.040382	2.507372
209.059421	1997.977817	18.054400	-0.040369	2.502887
208.916212	1990.046525	18.059405	-0.040337	2.498402
208.934994	1982.064458	18.064410	-0.040336	2.493892
208.954637	1974.098630	18.069415	-0.040334	2.489383
208.741510	1966.143317	18.074419	-0.040289	2.484854
208.854846	1958.190411	18.079424	-0.040305	2.480343
208.752085	1950.244673	18.084429	-0.040281	2.475812
208.611519	1942.269248	18.089434	-0.040250	2.471252
208.720604	1934.273320	18.094439	-0.040265	2.466691
208.419009	1926.346860	18.099443	-0.040204	2.462131
208.330045	1918.403907	18.104448	-0.040182	2.457568
208.328881	1910.436020	18.109453	-0.040177	2.452989
208.179604	1902.456935	18.114458	-0.040144	2.448384
208.109989	1894.521140	18.119463	-0.040126	2.443802
208.063205	1886.544368	18.124467	-0.040112	2.439188
208.125026	1878.589939	18.129472	-0.040118	2.434588
208.246205	1870.536738	18.134477	-0.040135	2.429925
207.939812	1862.604005	18.139482	-0.040073	2.425292
207.907440	1854.663729	18.144487	-0.040062	2.420665
207.919478	1846.688918	18.149491	-0.040059	2.416014
207.508199	1838.778726	18.154496	-0.039977	2.411358
207.665859	1830.778054	18.159501	-0.040002	2.406684
207.783355	1822.800287	18.164506	-0.040018	2.402012
207.589400	1814.898857	18.169511	-0.039977	2.397351
207.413229	1806.935092	18.174515	-0.039939	2.392645
207.427637	1798.971646	18.179520	-0.039937	2.387946
207.408404	1791.008854	18.184525	-0.039928	2.383235
207.061973	1783.089120	18.189530	-0.039858	2.378514
207.186105	1775.120540	18.194535	-0.039876	2.373792
207.223530	1767.104168	18.199539	-0.039878	2.369025
207.354468	1759.140734	18.204544	-0.039897	2.364288
207.062319	1751.255201	18.209549	-0.039838	2.359554
207.089132	1743.291523	18.214554	-0.039838	2.354789
207.122206	1735.286931	18.219559	-0.039839	2.349990
206.742311	1727.362390	18.224563	-0.039763	2.345197
206.628837	1719.419959	18.229568	-0.039736	2.340404
206.790696	1711.447151	18.234573	-0.039761	2.335605
206.871777	1703.446676	18.239578	-0.039771	2.330774
206.795992	1695.525784	18.244583	-0.039752	2.325967
206.651498	1687.583686	18.249587	-0.039720	2.321133
206.590061	1679.657892	18.254592	-0.039703	2.316304
206.481708	1671.685773	18.259597	-0.039678	2.311434
206.318746	1663.731877	18.264602	-0.039643	2.306560
206.460017	1655.780393	18.269607	-0.039664	2.301702
206.237543	1647.841953	18.274611	-0.039617	2.296812
206.108794	1639.892450	18.279616	-0.039588	2.291912
206.026689	1631.939679	18.284621	-0.039568	2.287003
205.995196	1623.973058	18.289626	-0.039557	2.282080
206.051202	1616.040769	18.294631	-0.039562	2.277175
205.971995	1608.042424	18.299635	-0.039542	2.272207
205.832258	1600.058463	18.304640	-0.039511	2.267231
205.615575	1592.142330	18.309645	-0.039465	2.262280
205.594063	1584.175839	18.314650	-0.039456	2.257304
205.596902	1576.246702	18.319655	-0.039452	2.252342
205.586425	1568.278452	18.324659	-0.039445	2.247344
205.616361	1560.328486	18.329664	-0.039445	2.242349
205.595441	1552.409738	18.334669	-0.039436	2.237359
205.109527	1544.502342	18.339674	-0.039340	2.232323
205.181856	1536.536140	18.344679	-0.039349	2.227288
205.071414	1528.584272	18.349683	-0.039323	2.222235
205.143221	1520.628876	18.354688	-0.039331	2.217184
205.050697	1512.688719	18.359693	-0.039309	2.212116
204.921591	1504.736559	18.364698	-0.039280	2.207026
205.196557	1496.772130	18.369703	-0.039326	2.201953
204.915222	1488.862136	18.374707	-0.039268	2.196853
204.816980	1480.916431	18.379712	-0.039245	2.191734
204.869980	1472.929947	18.384717	-0.039249	2.186591
204.803513	1464.996757	18.389722	-0.039232	2.181459
204.621795	1457.090929	18.394727	-0.039193	2.176322
204.485921	1449.133715	18.399731	-0.039163	2.171144
204.528213	1441.182653	18.404736	-0.039165	2.165974
204.386168	1433.270358	18.409741	-0.039134	2.160800
204.230717	1425.344916	18.414746	-0.039100	2.155603
204.286248	1417.387583	18.419751	-0.039105	2.150393
204.207986	1409.433512	18.424755	-0.039085	2.145159
204.067593	1401.513714	18.429760	-0.039054	2.139930
203.883495	1393.606647	18.434765	-0.039014	2.134692
203.914861	1385.622179	18.439770	-0.039015	2.129410
203.919586	1377.697028	18.444775	-0.039011	2.124152
203.843769	1369.766521	18.449779	-0.038992	2.118869
203.873312	1361.812800	18.454784	-0.038992	2.113568
203.739334	1353.822865	18.459789	-0.038962	2.108214
203.514481	1345.909259	18.464794	-0.038915	2.102888
203.558490	1337.988029	18.469799	-0.038918	2.097570
203.378762	1330.060048	18.474803	-0.038879	2.092212
203.350806	1322.115668	18.479808	-0.038869	2.086844
203.462494	1314.173028	18.484813	-0.038885	2.081477
203.283720	1306.268044	18.489818	-0.038846	2.076093
203.226666	1298.340045	18.494823	-0.038830	2.070691
203.356446	1290.370744	18.499827	-0.038849	2.065266
203.256591	1282.459260	18.504832	-0.038826	2.059843
202.972535	1274.585638	18.509837	-0.038768	2.054413
202.716782	1266.641848	18.514842	-0.038715	2.048923
202.846503	1258.700679	18.519847	-0.038734	2.043459
202.674664	1250.786632	18.524851	-0.038697	2.037969
202.589508	1242.848439	18.529856	-0.038676	2.032456
202.559637	1234.901260	18.534861	-0.038665	2.026927
202.462850	1226.966408	18.539866	-0.038642	2.021385
202.363182	1219.072747	18.544871	-0.038618	2.015856
202.482284	1211.081706	18.549875	-0.038635	2.010266
202.363069	1203.181338	18.554880	-0.038608	2.004699
202.543276	1195.254585	18.559885	-0.038637	1.999130
202.246366	1187.359317	18.564890	-0.038576	1.993518
202.278241	1179.427922	18.569895	-0.038577	1.987898
202.175916	1171.511039	18.574899	-0.038553	1.982259
201.841024	1163.625618	18.579904	-0.038485	1.976601
201.871158	1155.682578	18.584909	-0.038486	1.970925
201.630980	1147.779952	18.589914	-0.038436	1.965232
201.695277	1139.851781	18.594919	-0.038443	1.959538
201.549700	1131.934594	18.599923	-0.038411	1.953811
201.596809	1123.951028	18.604928	-0.038414	1.948041
201.700935	1116.020720	18.609933	-0.038428	1.942299
201.375734	1108.150707	18.614938	-0.038363	1.936536
201.399467	1100.225102	18.619943	-0.038362	1.930754
201.247237	1092.311404	18.624947	-0.038329	1.924944
201.074270	1084.435439	18.629952	-0.038291	1.919141
201.146438	1076.500205	18.634957	-0.038300	1.913305
201.050017	1068.576850	18.639962	-0.038276	1.907441
201.031620	1060.678492	18.644967	-0.038268	1.901585
200.899167	1052.769126	18.649971	-0.038238	1.895691
200.803705	1044.852689	18.654976	-0.038215	1.889777
200.977627	1036.925089	18.659981	-0.038243	1.883867
200.794942	1029.041204	18.664986	-0.038203	1.877930
200.845016	1021.130920	18.669991	-0.038208	1.871982
200.445021	1013.237876	18.674995	-0.038128	1.865975
200.458209	1005.319918	18.680000	-0.038125	1.859978
200.332453	997.443187	18.685005	-0.038097	1.853977
200.220599	989.517139	18.690010	-0.038071	1.847920
200.328372	981.611333	18.695015	-0.038086	1.841885
200.394620	973.698296	18.700019	-0.038093	1.835819
200.323680	965.800450	18.705024	-0.038075	1.829728
200.048364	957.941050	18.710029	-0.038018	1.823623
199.921803	950.039999	18.715034	-0.037990	1.817482
200.131696	942.119564	18.720039	-0.038024	1.811347
200.071908	934.216730	18.725043	-0.038007	1.805171
199.761783	926.380706	18.730048	-0.037945	1.798996
199.712301	918.467374	18.735053	-0.037930	1.792771
199.600741	910.528334	18.740058	-0.037904	1.786496
199.757481	902.625753	18.745063	-0.037928	1.780261
199.418540	894.781885	18.750067	-0.037860	1.773989
199.270581	886.894042	18.755072	-0.037828	1.767684
199.156216	879.011467	18.760077	-0.037801	1.761364
199.071748	871.134909	18.765082	-0.037780	1.755030
199.110673	863.236578	18.770087	-0.037783	1.748672
198.810635	855.370628	18.775091	-0.037722	1.742273
198.820110	847.484143	18.780096	-0.037718	1.735873
198.705079	839.597256	18.785101	-0.037692	1.729434
198.685528	831.710319	18.790106	-0.037683	1.722982
198.870985	823.821585	18.795111	-0.037712	1.716532
198.629620	815.947800	18.800115	-0.037662	1.710013
198.590369	808.064243	18.805120	-0.037650	1.703489
198.659431	800.185702	18.810125	-0.037658	1.696957
198.407027	792.317895	18.815130	-0.037606	1.690367
198.360556	784.465131	18.820135	-0.037592	1.683791
198.211636	776.623468	18.825139	-0.037559	1.677184
198.056400	768.748948	18.830144	-0.037525	1.670523
198.119160	760.863210	18.835149	-0.037532	1.663855
198.092526	752.994034	18.840154	-0.037522	1.657163
197.928794	745.155260	18.845159	-0.037486	1.650450
197.898636	737.278654	18.850163	-0.037475	1.643696
198.013831	729.411916	18.855168	-0.037492	1.636942
197.908789	721.519266	18.860173	-0.037467	1.630107
197.594308	713.681596	18.865178	-0.037403	1.623263
197.592989	705.832808	18.870183	-0.037398	1.616423
197.487013	697.974860	18.875187	-0.037373	1.609532
197.354853	690.139039	18.880192	-0.037344	1.602626
197.243595	682.311994	18.885197	-0.037318	1.595702
197.216034	674.441726	18.890202	-0.037308	1.588720
197.202159	666.598553	18.895207	-0.037300	1.581734
196.914765	658.787768	18.900211	-0.037241	1.574707
196.847929	650.933649	18.905216	-0.037224	1.567641
196.911003	643.085648	18.910221	-0.037230	1.560567
196.632728	635.285559	18.915226	-0.037174	1.553455
196.730361	627.406466	18.920231	-0.037187	1.546293
196.560654	619.590547	18.925235	-0.037150	1.539116
196.531657	611.749033	18.930240	-0.037140	1.531903
196.445742	603.926677	18.935245	-0.037119	1.524665
196.386095	596.103473	18.940250	-0.037102	1.517396
196.335501	588.283364	18.945255	-0.037088	1.510096
196.074469	580.485526	18.950259	-0.037034	1.502749
196.126551	572.660325	18.955264	-0.037039	1.495388
196.062902	564.838785	18.960269	-0.037022	1.487976
195.835489	557.046829	18.965274	-0.036975	1.480530
195.739691	549.248723	18.970279	-0.036952	1.473061
195.786294	541.364549	18.975283	-0.036955	1.465493
195.508203	533.605408	18.980288	-0.036898	1.457956
195.402157	525.804916	18.985293	-0.036874	1.450366
195.297287	517.997859	18.990298	-0.036849	1.442731
195.285531	510.219338	18.995303	-0.036842	1.435098
195.118081	502.428571	19.000307	-0.036806	1.427386
194.931923	494.657349	19.005312	-0.036766	1.419649
195.026190	486.856765	19.010317	-0.036778	1.411887
194.672493	479.104420	19.015322	-0.036708	1.404055
194.593897	471.342940	19.020327	-0.036688	1.396216
194.352724	463.559909	19.025331	-0.036638	1.388284
194.563629	455.728552	19.030336	-0.036672	1.380333
194.423974	447.986883	19.035341	-0.036641	1.372369
194.237469	440.221222	19.040346	-0.036601	1.364325
194.192148	432.474030	19.045351	-0.036588	1.356277
194.156856	424.698172	19.050355	-0.036576	1.348153
193.921097	416.974001	19.055360	-0.036527	1.339999
193.860073	409.229502	19.060365	-0.036511	1.331804
193.790228	401.471664	19.065370	-0.036493	1.323542
193.553832	393.768690	19.070375	-0.036444	1.315258
193.541296	385.879600	19.075379	-0.036437	1.306760
193.324318	378.182557	19.080384	-0.036391	1.298378
193.202104	370.472852	19.085389	-0.036363	1.289945
192.942008	362.778423	19.090394	-0.036310	1.281448
192.922781	355.068229	19.095399	-0.036302	1.272922
192.422963	347.413309	19.100403	-0.036203	1.264309
192.258572	339.721668	19.105408	-0.036168	1.255660
192.230733	332.005800	19.110413	-0.036158	1.246949
191.779827	324.361970	19.115418	-0.036069	1.238177
191.328855	316.710984	19.120423	-0.035980	1.229334
191.083469	309.020139	19.125427	-0.035929	1.220421
190.991860	301.327849	19.130432	-0.035907	1.211471
190.405233	293.725169	19.135437	-0.035793	1.202461
190.013407	286.088256	19.140442	-0.035715	1.193382
189.847729	278.416270	19.145447	-0.035679	1.184236
189.498482	270.788546	19.150451	-0.035609	1.175035
189.128499	263.156928	19.155456	-0.035536	1.165753
188.984433	255.526551	19.160461	-0.035504	1.156444
188.314375	247.909968	19.165466	-0.035374	1.146965
187.856430	240.327444	19.170471	-0.035284	1.137495
187.710864	232.680246	19.175475	-0.035252	1.127931
187.178462	225.124355	19.180480	-0.035148	1.118317
186.745243	217.554321	19.185485	-0.035062	1.108623
186.284178	209.983768	19.190490	-0.034972	1.098836
186.096001	202.388803	19.195495	-0.034932	1.088991
185.659256	194.849686	19.200499	-0.034845	1.079072
184.893916	187.352309	19.205504	-0.034698	1.069041
184.587679	179.794002	19.210509	-0.034636	1.058940
184.049917	172.276331	19.215514	-0.034531	1.048742
183.593239	164.780753	19.220519	-0.034441	1.038492
183.237978	157.254523	19.225523	-0.034370	1.028122
183.206152	149.697343	19.230528	-0.034359	1.017682
182.737864	142.232789	19.235533	-0.034267	1.007156
182.265566	134.784110	19.240538	-0.034175	0.996541
181.830582	127.299444	19.245543	-0.034089	0.985769
181.121674	119.910338	19.250547	-0.033952	0.974946
180.610435	112.486649	19.255552	-0.033852	0.964002
180.269475	105.066069	19.260557	-0.033784	0.952981
179.754276	97.677677	19.265562	-0.033683	0.941833
179.342040	90.302978	19.270567	-0.033601	0.930599
179.061857	82.909448	19.275571	-0.033545	0.919234
178.643248	75.551592	19.280576	-0.033462	0.907745
178.166779	68.235368	19.285581	-0.033368	0.896158
177.497459	61.182292	19.290586	-0.033239	0.884784