Thu Mar 11 20:26:19 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.918400	-0.097204	0.000000	-0.000035	0.722079

0.673636	-0.053259	0.005005	0.000011	0.722080
0.573583	-0.033015	0.010010	0.000029	0.722084
0.544892	-0.032511	0.015014	0.000035	0.722076
0.641014	-0.044815	0.020019	0.000017	0.722085
0.603541	-0.040959	0.025024	0.000024	0.722080
0.793249	-0.075052	0.030029	-0.000012	0.722079
0.991932	-0.108280	0.035034	-0.000049	0.722084
0.733287	-0.066154	0.040038	-0.000001	0.722076
0.501556	-0.022901	0.045043	0.000042	0.722080
0.649340	-0.051635	0.050048	0.000015	0.722076
0.978971	-0.110405	0.055053	-0.000047	0.722076
1.040384	-0.117164	0.060058	-0.000058	0.722084
0.781329	-0.075998	0.065062	-0.000010	0.722074
1.080321	-0.123710	0.070067	-0.000066	0.722085
0.907502	-0.182801	0.075072	-0.000034	0.721909
0.910767	-0.266035	0.080077	-0.000034	0.721747
0.972190	-0.273712	0.085082	-0.000046	0.721753
0.473334	-0.188294	0.090086	0.000047	0.721747
0.323899	-0.159059	0.095091	0.000075	0.721752
0.522872	-0.197305	0.100096	0.000037	0.721747
0.685528	-0.228289	0.105101	0.000007	0.721743
0.731612	-0.357523	0.110106	-0.000001	0.721505
0.618506	-0.371004	0.115110	0.000020	0.721439
0.675899	-0.378043	0.120115	0.000009	0.721445
0.357874	-0.324624	0.125120	0.000068	0.721439
0.597793	-0.366786	0.130125	0.000023	0.721441
0.837223	-0.505198	0.135130	-0.000021	0.721252
0.878194	-0.577929	0.140134	-0.000029	0.721124
0.656106	-0.535401	0.145139	0.000012	0.721130
0.646254	-0.535785	0.150144	0.000014	0.721126
0.692599	-0.605733	0.155149	0.000005	0.721005
0.727866	-0.671396	0.160154	-0.000001	0.720888
0.224222	-0.586862	0.165158	0.000092	0.720878
0.450681	-0.623337	0.170163	0.000050	0.720886
0.255947	-0.686343	0.175168	0.000086	0.720694
0.107867	-0.736618	0.180173	0.000114	0.720543
0.321187	-0.770161	0.185178	0.000074	0.720552
0.347289	-0.779840	0.190182	0.000069	0.720542
0.180449	-0.890335	0.195187	0.000100	0.720266
0.165058	-0.906098	0.200192	0.000103	0.720230
0.275171	-0.926893	0.205197	0.000082	0.720228
0.458993	-1.047001	0.210202	0.000048	0.720056
0.286001	-1.094236	0.215206	0.000080	0.719902
0.508528	-1.130098	0.220211	0.000039	0.719910
0.337162	-1.189924	0.225216	0.000071	0.719732
-0.134957	-1.170428	0.230221	0.000159	0.719605
0.299179	-1.244335	0.235226	0.000078	0.719611
0.213218	-1.349694	0.240230	0.000094	0.719374
0.065505	-1.372702	0.245235	0.000121	0.719277
-0.227412	-1.323063	0.250240	0.000176	0.719272
-0.087279	-1.484299	0.255245	0.000149	0.719003
0.059020	-1.527481	0.260250	0.000122	0.718969
-0.282036	-1.504080	0.265254	0.000186	0.718896
-0.287907	-1.626705	0.270259	0.000187	0.718652
-0.178046	-1.648324	0.275264	0.000166	0.718648
-0.189915	-1.739676	0.280269	0.000168	0.718464
-0.553996	-1.724794	0.285274	0.000236	0.718365
-0.437065	-1.765024	0.290278	0.000214	0.718327
-0.611034	-1.885822	0.295283	0.000247	0.718028
-0.556104	-1.897696	0.300288	0.000236	0.718024
-0.452565	-2.018962	0.305293	0.000217	0.717821
-0.622133	-2.045312	0.310298	0.000249	0.717709
-1.012978	-2.016485	0.315302	0.000321	0.717628
-0.818378	-2.173257	0.320307	0.000285	0.717387
-2.093556	-1.947303	0.325312	0.000522	0.717385
-1.956954	-2.071838	0.330317	0.000497	0.717187
-2.776154	-1.973227	0.335322	0.000649	0.717094
-2.889364	-1.959016	0.340326	0.000670	0.717082
-2.651124	-2.111946	0.345331	0.000626	0.716863
-3.868506	-1.947628	0.350336	0.000852	0.716760
-4.006273	-1.927028	0.355341	0.000878	0.716752
-3.679181	-2.028665	0.360346	0.000817	0.716666
-5.023915	-1.901366	0.365350	0.001067	0.716444
-4.688799	-1.957116	0.370355	0.001005	0.716452
-4.634073	-1.966663	0.375360	0.000995	0.716453
-4.791583	-2.008997	0.380365	0.001024	0.716314
-5.566029	-1.958046	0.385370	0.001168	0.716141
-5.524392	-1.969597	0.390374	0.001160	0.716133
-5.379058	-1.993355	0.395379	0.001133	0.716138
-5.216074	-2.061744	0.400384	0.001103	0.716060
-6.167555	-1.981152	0.405389	0.001280	0.715884
-5.960962	-2.015470	0.410394	0.001241	0.715889
-6.293362	-1.960349	0.415398	0.001303	0.715881
-6.487566	-1.922087	0.420403	0.001339	0.715888
-6.701767	-2.039979	0.425408	0.001379	0.715579
-7.409558	-1.931091	0.430413	0.001510	0.715545
-7.250711	-1.955370	0.435418	0.001481	0.715553
-7.227248	-1.965018	0.440422	0.001476	0.715543
-7.276095	-1.952691	0.445427	0.001485	0.715550
-7.580170	-2.043004	0.450432	0.001542	0.715264
-8.198916	-1.949221	0.455437	0.001657	0.715231
-8.089285	-1.964419	0.460442	0.001637	0.715240
-8.122209	-1.963390	0.465446	0.001643	0.715231
-8.081114	-1.966891	0.470451	0.001635	0.715238
-8.178929	-2.032242	0.475456	0.001653	0.715074
-9.364086	-1.906577	0.480461	0.001874	0.714905
-8.784446	-2.005314	0.485466	0.001766	0.714914
-9.089282	-1.954150	0.490470	0.001822	0.714908
-8.886110	-1.987628	0.495475	0.001784	0.714913
-8.731871	-2.014748	0.500480	0.001756	0.714914
-9.690556	-1.966956	0.505485	0.001934	0.714670
-10.017041	-1.935522	0.510490	0.001995	0.714617
-9.880106	-1.965064	0.515494	0.001969	0.714607
-9.625138	-2.007732	0.520499	0.001922	0.714613
-9.966303	-1.947656	0.525504	0.001985	0.714612
-9.851013	-1.971062	0.530509	0.001963	0.714606
-9.646119	-2.106694	0.535514	0.001925	0.714409
-11.217208	-1.893869	0.540518	0.002218	0.714276
-10.836666	-1.958598	0.545523	0.002147	0.714283
-10.358473	-2.043160	0.550528	0.002058	0.714284
-11.005059	-1.931184	0.555533	0.002178	0.714278
-10.666200	-1.987268	0.560538	0.002115	0.714286
-10.667653	-2.036041	0.565542	0.002115	0.714189
-11.884607	-1.927564	0.570547	0.002341	0.713974
-11.796189	-1.943824	0.575552	0.002325	0.713973
-11.929172	-1.922131	0.580557	0.002350	0.713969
-11.669472	-1.961995	0.585562	0.002301	0.713982
-11.874447	-1.931246	0.590566	0.002339	0.713971
-11.933521	-1.918675	0.595571	0.002350	0.713975
-11.744264	-1.987973	0.600576	0.002315	0.713905
-12.739287	-1.938026	0.605581	0.002500	0.713652
-12.367759	-1.999663	0.610586	0.002431	0.713661
-12.657152	-1.951711	0.615590	0.002485	0.713654
-12.655360	-1.951791	0.620595	0.002484	0.713654
-12.723943	-1.937920	0.625600	0.002497	0.713658
-12.972460	-1.895680	0.630605	0.002543	0.713654
-12.447677	-2.028667	0.635610	0.002445	0.713576
-13.652150	-1.920619	0.640614	0.002669	0.713364
-13.581317	-1.931392	0.645619	0.002656	0.713368
-13.159181	-2.006836	0.650624	0.002578	0.713367
-13.575056	-1.935836	0.655629	0.002655	0.713361
-13.451879	-1.952913	0.660634	0.002632	0.713371
-13.578568	-1.936930	0.665638	0.002655	0.713358
-13.772450	-1.967202	0.670643	0.002691	0.713229
-14.754532	-1.893659	0.675648	0.002874	0.713028
-14.333563	-1.970583	0.680653	0.002796	0.713024
-14.378953	-1.958806	0.685658	0.002804	0.713032
-14.645995	-1.915693	0.690662	0.002854	0.713023
-14.303449	-1.972605	0.695667	0.002790	0.713031
-14.127883	-2.003805	0.700672	0.002757	0.713031
-14.497987	-1.999627	0.705677	0.002826	0.712909
-15.422032	-1.929434	0.710682	0.002998	0.712721
-14.983130	-2.013632	0.715686	0.002916	0.712709
-15.091074	-1.990005	0.720691	0.002936	0.712718
-15.166283	-1.977816	0.725696	0.002950	0.712716
-15.619625	-1.901114	0.730701	0.003034	0.712708
-15.171790	-1.974006	0.735706	0.002951	0.712722
-15.306841	-2.028534	0.740710	0.002976	0.712565
-16.241324	-1.947418	0.745715	0.003150	0.712395
-16.061964	-1.980040	0.750720	0.003117	0.712394
-16.463083	-1.911503	0.755725	0.003191	0.712388
-16.452925	-1.910528	0.760730	0.003189	0.712394
-16.130945	-1.972637	0.765734	0.003129	0.712385
-16.255730	-1.947696	0.770739	0.003152	0.712390
-16.404275	-1.947242	0.775744	0.003180	0.712339
-17.169624	-1.936732	0.780749	0.003322	0.712088
-16.460024	-2.059684	0.785754	0.003190	0.712095
-17.062258	-1.956601	0.790758	0.003302	0.712087
-17.302641	-1.911297	0.795763	0.003347	0.712092
-16.867326	-1.988117	0.800768	0.003266	0.712094
-16.903913	-1.984885	0.805773	0.003272	0.712087
-16.968556	-2.038492	0.810778	0.003284	0.711958
-18.306627	-1.900411	0.815782	0.003533	0.711758
-17.813657	-1.986214	0.820787	0.003442	0.711762
-18.029425	-1.947959	0.825792	0.003482	0.711762
-18.386293	-1.885814	0.830797	0.003548	0.711759
-17.730507	-1.998594	0.835802	0.003426	0.711767
-18.097333	-1.938707	0.840806	0.003494	0.711756
-18.103671	-1.945443	0.845811	0.003495	0.711741
-18.474784	-2.021855	0.850816	0.003564	0.711457
-18.989853	-1.933748	0.855821	0.003660	0.711450
-19.050721	-1.917851	0.860826	0.003671	0.711460
-18.587398	-2.003657	0.865830	0.003585	0.711454
-18.430531	-2.030041	0.870835	0.003556	0.711457
-18.635111	-1.992214	0.875840	0.003594	0.711460
-18.897475	-1.997382	0.880845	0.003642	0.711356
-19.532004	-1.989303	0.885850	0.003761	0.711147
-19.391145	-2.020072	0.890854	0.003734	0.711136
-19.787760	-1.947477	0.895859	0.003808	0.711140
-19.671551	-1.966930	0.900864	0.003786	0.711142
-19.458540	-2.008523	0.905869	0.003747	0.711135
-19.948077	-1.917257	0.910874	0.003838	0.711144
-20.026446	-1.946935	0.915878	0.003852	0.711057
-20.223360	-2.002677	0.920883	0.003889	0.710875
-20.195282	-2.008069	0.925888	0.003883	0.710875
-20.909000	-1.882640	0.930893	0.004016	0.710871
-20.353985	-1.975911	0.935898	0.003913	0.710883
-19.913862	-2.060399	0.940902	0.003831	0.710871
-20.363271	-1.977847	0.945907	0.003914	0.710876
-20.693180	-2.062120	0.950912	0.003976	0.710591
-21.435337	-1.958702	0.955917	0.004114	0.710533
-21.441604	-1.953283	0.960922	0.004115	0.710542
-21.548110	-1.938872	0.965926	0.004135	0.710533
-21.501353	-1.944388	0.970931	0.004126	0.710539
-21.253115	-1.987880	0.975936	0.004080	0.710540
-21.667965	-1.917778	0.980941	0.004157	0.710533
-21.619233	-2.029843	0.985946	0.004148	0.710326
-22.463730	-1.934070	0.990950	0.004305	0.710217
-22.123501	-1.993097	0.995955	0.004241	0.710221
-22.029969	-2.008239	1.000960	0.004224	0.710224
-22.529393	-1.923375	1.005965	0.004317	0.710216
-22.125336	-1.990613	1.010970	0.004241	0.710225
-22.499108	-1.927594	1.015974	0.004311	0.710218
-22.708939	-2.004465	1.020979	0.004350	0.709990
-23.175124	-1.970148	1.025984	0.004437	0.709893
-23.361212	-1.940612	1.030989	0.004471	0.709886
-22.693053	-2.054648	1.035994	0.004347	0.709896
-23.112085	-1.981647	1.040998	0.004425	0.709893
-23.314451	-1.942885	1.046003	0.004462	0.709898
-23.422720	-1.924798	1.051008	0.004482	0.709896
-23.284686	-2.041089	1.056013	0.004457	0.709713
-23.927274	-1.981478	1.061018	0.004576	0.709603
-24.018717	-1.969627	1.066022	0.004593	0.709594
-23.973457	-1.975856	1.071027	0.004585	0.709598
-23.775291	-2.010897	1.076032	0.004548	0.709599
-24.344312	-1.910577	1.081037	0.004653	0.709597
-24.014323	-1.967082	1.086042	0.004592	0.709602
-24.185697	-2.058270	1.091046	0.004624	0.709358
-25.152439	-1.932782	1.096051	0.004804	0.709265
-25.058362	-1.947986	1.101056	0.004786	0.709268
-24.740974	-2.007357	1.106061	0.004727	0.709263
-24.852401	-1.983166	1.111066	0.004748	0.709271
-25.328944	-1.901938	1.116070	0.004836	0.709264
-24.999702	-1.959326	1.121075	0.004775	0.709267
-24.696475	-2.093939	1.126080	0.004718	0.709106
-26.033635	-1.932824	1.131085	0.004967	0.708951
-25.701035	-1.987772	1.136090	0.004905	0.708960
-25.902480	-1.954790	1.141094	0.004943	0.708954
-25.909952	-1.952325	1.146099	0.004944	0.708957
-25.980395	-1.938481	1.151104	0.004957	0.708960
-25.859598	-1.962464	1.156109	0.004934	0.708955
-25.635892	-2.073280	1.161114	0.004893	0.708813
-26.878014	-1.939158	1.166118	0.005124	0.708638
-26.582132	-1.990799	1.171123	0.005069	0.708641
-26.392821	-2.023913	1.176128	0.005033	0.708642
-27.150369	-1.893764	1.181133	0.005174	0.708633
-26.542224	-1.996422	1.186138	0.005061	0.708644
-26.353811	-2.033001	1.191142	0.005026	0.708638
-26.940324	-2.028053	1.196147	0.005135	0.708439
-27.716469	-1.931631	1.201152	0.005279	0.708355
-27.694916	-1.939209	1.206157	0.005275	0.708348
-27.250222	-2.016752	1.211162	0.005193	0.708351
-27.607206	-1.955265	1.216166	0.005259	0.708347
-27.887831	-1.903142	1.221171	0.005311	0.708352
-27.479634	-1.973518	1.226176	0.005235	0.708357
-27.801483	-2.009935	1.231181	0.005295	0.708169
-28.680455	-1.930907	1.236186	0.005458	0.708013
-28.245626	-2.010821	1.241190	0.005377	0.708009
-28.365824	-1.987214	1.246195	0.005400	0.708013
-28.496181	-1.963510	1.251200	0.005424	0.708014
-28.513697	-1.962683	1.256205	0.005427	0.708010
-28.024821	-2.046429	1.261210	0.005336	0.708017
-28.483546	-2.061632	1.266214	0.005421	0.707822
-29.695639	-1.906686	1.271219	0.005647	0.707700
-29.073799	-2.015809	1.276224	0.005531	0.707704
-29.351781	-1.971356	1.281229	0.005583	0.707694
-29.514721	-1.935968	1.286234	0.005613	0.707706
-29.307176	-1.977317	1.291238	0.005574	0.707698
-29.280185	-1.979245	1.296243	0.005569	0.707704
-29.449889	-2.029305	1.301248	0.005601	0.707543
-30.522298	-1.923460	1.306253	0.005800	0.707372
-29.913612	-2.027246	1.311258	0.005687	0.707381
-30.025990	-2.010130	1.316262	0.005708	0.707376
-30.509752	-1.923122	1.321267	0.005798	0.707377
-29.946695	-2.020875	1.326272	0.005693	0.707383
-30.298804	-1.963634	1.331277	0.005758	0.707372
-30.651804	-1.972698	1.336282	0.005824	0.707228
-31.378986	-1.917809	1.341286	0.005959	0.707078
-30.835767	-2.013935	1.346291	0.005858	0.707079
-30.872747	-2.004347	1.351296	0.005865	0.707086
-31.511372	-1.895992	1.356301	0.005984	0.707075
-30.866351	-2.005832	1.361306	0.005864	0.707085
-31.175167	-1.953311	1.366310	0.005921	0.707080
-31.283678	-1.980967	1.371315	0.005941	0.706986
-31.621278	-2.035638	1.376320	0.006004	0.706756
-31.778454	-2.010494	1.381325	0.006033	0.706750
-32.148291	-1.941458	1.386330	0.006102	0.706756
-32.167060	-1.940092	1.391334	0.006105	0.706752
-31.904873	-1.986903	1.396339	0.006056	0.706752
-31.950526	-1.976781	1.401344	0.006065	0.706757
-32.341900	-1.948398	1.406349	0.006138	0.706674
-32.692107	-1.996688	1.411354	0.006203	0.706451
-32.658879	-2.007425	1.416358	0.006196	0.706442
-33.129900	-1.921634	1.421363	0.006284	0.706446
-32.808165	-1.977624	1.426368	0.006224	0.706449
-32.934560	-1.958431	1.431373	0.006247	0.706442
-33.023441	-1.938584	1.436378	0.006264	0.706450
-33.045590	-1.945470	1.441382	0.006268	0.706429
-33.389097	-2.033856	1.446387	0.006332	0.706128
-33.561749	-1.999699	1.451392	0.006364	0.706135
-33.979347	-1.929410	1.456397	0.006442	0.706127
-33.498222	-2.012183	1.461402	0.006352	0.706133
-33.476380	-2.019374	1.466406	0.006348	0.706126
-33.917819	-1.939477	1.471411	0.006430	0.706129
-33.649629	-2.022067	1.476416	0.006380	0.706059
-34.527685	-1.964904	1.481421	0.006543	0.705860
-34.381536	-1.986841	1.486426	0.006516	0.705868
-34.880867	-1.902173	1.491430	0.006609	0.705859
-34.720951	-1.928854	1.496435	0.006579	0.705863
-34.171016	-2.025798	1.501440	0.006477	0.705866
-34.701458	-1.934381	1.506445	0.006575	0.705859
-34.509254	-2.032397	1.511450	0.006539	0.705731
-35.571131	-1.946292	1.516454	0.006737	0.705524
-35.599013	-1.941320	1.521459	0.006742	0.705524
-35.655833	-1.928473	1.526464	0.006753	0.705530
-35.587466	-1.945856	1.531469	0.006740	0.705519
-35.305597	-1.990982	1.536474	0.006687	0.705530
-35.548304	-1.949962	1.541478	0.006732	0.705525
-35.627761	-1.970897	1.546483	0.006747	0.705455
-36.222168	-1.984095	1.551488	0.006858	0.705215
-36.655455	-1.912045	1.556493	0.006938	0.705205
-36.576570	-1.921841	1.561498	0.006924	0.705214
-36.219010	-1.988644	1.566502	0.006857	0.705208
-36.414302	-1.952043	1.571507	0.006893	0.705211
-36.467693	-1.940895	1.576512	0.006903	0.705215
-36.171094	-2.013191	1.581517	0.006848	0.705176
-36.943704	-2.015458	1.586522	0.006992	0.704894
-37.156063	-1.980193	1.591526	0.007031	0.704889
-37.388719	-1.938133	1.596531	0.007074	0.704890
-36.754552	-2.049598	1.601536	0.006956	0.704894
-37.375402	-1.942169	1.606541	0.007072	0.704887
-37.193142	-1.970435	1.611546	0.007038	0.704896
-37.348102	-1.988067	1.616550	0.007066	0.704805
-38.289830	-1.926327	1.621555	0.007242	0.704591
-38.182240	-1.943065	1.626560	0.007222	0.704596
-38.270875	-1.929895	1.631565	0.007238	0.704591
-38.223522	-1.936088	1.636570	0.007229	0.704596
-38.220168	-1.940984	1.641574	0.007228	0.704587
-38.226615	-1.939290	1.646579	0.007229	0.704589
-37.892368	-2.009800	1.651584	0.007167	0.704567
-39.028278	-1.960288	1.656589	0.007379	0.704259
-39.063417	-1.948640	1.661594	0.007385	0.704270
-39.051473	-1.953555	1.666598	0.007383	0.704264
-39.109699	-1.944720	1.671603	0.007394	0.704261
-39.088912	-1.945094	1.676608	0.007390	0.704268
-39.501857	-1.876659	1.681613	0.007466	0.704258
-39.042423	-1.955353	1.686618	0.007381	0.704264
-39.142577	-2.039110	1.691622	0.007399	0.704060
-40.187248	-1.904214	1.696627	0.007594	0.703956
-39.690608	-1.991596	1.701632	0.007501	0.703959
-39.861211	-1.965279	1.706637	0.007533	0.703951
-40.006502	-1.936781	1.711642	0.007560	0.703956
-39.726284	-1.989950	1.716646	0.007508	0.703950
-39.759693	-1.983566	1.721651	0.007514	0.703951
-40.514309	-1.997476	1.726656	0.007654	0.703651
-40.903164	-1.938473	1.731661	0.007727	0.703631
-40.831698	-1.945874	1.736666	0.007713	0.703642
-40.900815	-1.936566	1.741670	0.007726	0.703636
-40.995303	-1.920375	1.746675	0.007743	0.703635
-40.691999	-1.972632	1.751680	0.007687	0.703638
-40.858973	-1.946573	1.756685	0.007718	0.703631
-41.170654	-1.996851	1.761690	0.007776	0.703418
-41.785322	-1.924878	1.766694	0.007890	0.703342
-41.632651	-1.953798	1.771699	0.007862	0.703338
-41.393493	-1.995006	1.776704	0.007817	0.703342
-41.672419	-1.949177	1.781709	0.007869	0.703334
-41.364545	-1.997998	1.786714	0.007812	0.703346
-41.473951	-1.995384	1.791718	0.007832	0.703312
-42.473939	-1.968684	1.796723	0.008018	0.703006
-42.324343	-1.994118	1.801728	0.007990	0.703009
-42.833056	-1.905848	1.806733	0.008085	0.703004
-42.534249	-1.957654	1.811738	0.008029	0.703007
-42.610352	-1.944469	1.816742	0.008043	0.703007
-42.808834	-1.910585	1.821747	0.008080	0.703004
-42.612917	-1.941921	1.826752	0.008043	0.703011
-42.838405	-2.028057	1.831757	0.008085	0.702756
-43.563578	-1.928885	1.836762	0.008220	0.702695
-43.744126	-1.898159	1.841766	0.008254	0.702693
-43.394924	-1.961888	1.846771	0.008189	0.702690
-43.226644	-1.987410	1.851776	0.008157	0.702699
-43.229477	-1.990997	1.856781	0.008158	0.702691
-43.449139	-1.949125	1.861786	0.008199	0.702697
-44.038475	-1.984264	1.866790	0.008308	0.702413
-44.271321	-1.964905	1.871795	0.008351	0.702369
-44.181858	-1.978423	1.876800	0.008335	0.702374
-44.169880	-1.986425	1.881805	0.008332	0.702362
-44.206689	-1.973837	1.886810	0.008339	0.702374
-44.427012	-1.935824	1.891814	0.008380	0.702372
-44.318641	-1.955879	1.896819	0.008360	0.702371
-44.495891	-2.057210	1.901824	0.008393	0.702102
-45.130386	-1.959314	1.906829	0.008511	0.702071
-45.372590	-1.913346	1.911834	0.008556	0.702077
-45.034345	-1.974313	1.916838	0.008493	0.702076
-45.153358	-1.953360	1.921843	0.008515	0.702075
-45.181289	-1.946602	1.926848	0.008520	0.702079
-45.188333	-1.962517	1.931853	0.008521	0.702045
-45.594113	-2.035954	1.936858	0.008597	0.701750
-45.797962	-2.002187	1.941862	0.008635	0.701745
-46.237137	-1.925764	1.946867	0.008716	0.701741
-45.748696	-2.007728	1.951872	0.008625	0.701752
-45.867617	-1.990648	1.956877	0.008647	0.701743
-46.124408	-1.941231	1.961882	0.008695	0.701751
-45.960138	-2.017922	1.966886	0.008664	0.701655
-47.148344	-1.913625	1.971891	0.008886	0.701438
-46.824582	-1.966961	1.976896	0.008825	0.701447
-47.189192	-1.906531	1.981901	0.008893	0.701437
-46.800910	-1.973569	1.986906	0.008821	0.701442
-46.960830	-1.947749	1.991910	0.008850	0.701437
-47.504038	-1.850421	1.996915	0.008951	0.701438
-46.959060	-2.003179	2.001920	0.008850	0.701326

-47.888505	-1.935688	2.011917	0.009023	0.701127
-47.592049	-1.988279	2.021914	0.008967	0.701128
-47.781619	-1.955705	2.031910	0.009003	0.701126
-47.810912	-1.951326	2.041907	0.009008	0.701124
-47.792588	-1.954474	2.051904	0.009004	0.701125
-47.786948	-1.953623	2.061901	0.009003	0.701129
-47.640170	-1.980140	2.071898	0.008976	0.701128
-47.875459	-1.939375	2.081894	0.009019	0.701126
-47.615633	-1.986861	2.091891	0.008971	0.701124
-47.437393	-2.018101	2.101888	0.008937	0.701126
-47.816469	-1.923759	2.111885	0.009008	0.701180
-46.596621	-2.012870	2.121882	0.008781	0.701440
-46.791571	-1.979647	2.131878	0.008817	0.701438
-46.831121	-1.972513	2.141875	0.008824	0.701438
-46.928710	-1.954837	2.151872	0.008842	0.701439
-46.948908	-1.951038	2.161869	0.008845	0.701440
-46.839180	-1.936165	2.171866	0.008825	0.701510
-46.203978	-1.933470	2.181862	0.008706	0.701745
-46.031992	-1.964442	2.191859	0.008674	0.701744
-45.973407	-1.974614	2.201856	0.008663	0.701745
-46.215391	-1.920724	2.211853	0.008708	0.701767
-45.185454	-1.953054	2.221850	0.008516	0.702074
-45.129369	-1.963746	2.231846	0.008506	0.702073
-45.260700	-1.940981	2.241843	0.008530	0.702072
-45.049055	-1.967007	2.251840	0.008490	0.702096
-44.501375	-1.927880	2.261837	0.008388	0.702372
-44.200116	-1.982095	2.271834	0.008332	0.702372
-44.510743	-1.928057	2.281830	0.008390	0.702369
-44.279990	-1.915305	2.291827	0.008346	0.702479
-43.454493	-1.957117	2.301824	0.008193	0.702692
-43.446975	-1.956906	2.311821	0.008191	0.702695
-43.598522	-1.930306	2.321818	0.008219	0.702695
-42.811905	-1.937254	2.331814	0.008073	0.702964
-42.481019	-1.976707	2.341811	0.008011	0.703004
-42.489941	-1.973022	2.351808	0.008012	0.703009
-42.503681	-1.948473	2.361805	0.008015	0.703054
-41.776613	-1.933038	2.371802	0.007879	0.703347
-41.657639	-1.956220	2.381798	0.007857	0.703343
-41.617201	-1.963387	2.391795	0.007849	0.703344
-41.410027	-1.919749	2.401792	0.007810	0.703506
-40.573975	-2.003901	2.411789	0.007655	0.703638
-40.921951	-1.941933	2.421786	0.007719	0.703638
-40.696634	-1.983494	2.431782	0.007677	0.703635
-39.814438	-1.994500	2.441779	0.007513	0.703931
-40.039779	-1.945989	2.451776	0.007554	0.703948
-39.868730	-1.974155	2.461773	0.007522	0.703953
-39.927775	-1.898211	2.471770	0.007533	0.704085
-39.118948	-1.956204	2.481766	0.007383	0.704259
-39.077874	-1.964181	2.491763	0.007375	0.704258
-39.303148	-1.914128	2.501760	0.007416	0.704278
-38.215375	-1.955239	2.511757	0.007214	0.704587
-38.127012	-1.969552	2.521754	0.007197	0.704590
-38.107463	-1.974313	2.531750	0.007193	0.704588
-38.093456	-1.901865	2.541747	0.007191	0.704739
-37.261540	-1.978280	2.551744	0.007036	0.704884
-37.333198	-1.962629	2.561741	0.007049	0.704890
-37.330512	-1.961744	2.571738	0.007048	0.704893
-36.593462	-1.938202	2.581734	0.006911	0.705206
-36.562993	-1.943318	2.591731	0.006905	0.705207
-36.464859	-1.959371	2.601728	0.006886	0.705210
-35.975028	-1.955643	2.611725	0.006795	0.705393
-35.644009	-1.950570	2.621722	0.006733	0.705523
-35.462720	-1.981718	2.631718	0.006699	0.705525
-35.550278	-1.964861	2.641715	0.006716	0.705528
-34.886584	-1.915734	2.651712	0.006592	0.705865
-34.609865	-1.965174	2.661709	0.006540	0.705865
-34.770126	-1.937610	2.671706	0.006570	0.705864
-34.193750	-1.972188	2.681702	0.006462	0.706001
-34.137037	-1.918662	2.691699	0.006452	0.706129
-33.888254	-1.962616	2.701696	0.006405	0.706130
-33.989343	-1.911819	2.711693	0.006424	0.706196
-33.116448	-1.943568	2.721690	0.006261	0.706446
-32.835118	-1.993128	2.731686	0.006209	0.706447
-33.188761	-1.930900	2.741683	0.006274	0.706446
-32.395725	-1.954473	2.751680	0.006126	0.706683
-32.205898	-1.952744	2.761677	0.006091	0.706755
-31.979166	-1.992959	2.771674	0.006049	0.706755
-32.212363	-1.913680	2.781670	0.006092	0.706831
-31.472559	-1.921971	2.791667	0.005954	0.707080
-30.923175	-2.018569	2.801664	0.005852	0.707083
-31.465560	-1.920756	2.811661	0.005952	0.707085
-30.633467	-1.944396	2.821658	0.005797	0.707336
-30.325642	-1.977411	2.831654	0.005740	0.707380
-30.543515	-1.940752	2.841651	0.005780	0.707376
-30.202320	-1.942750	2.851648	0.005716	0.707494
-29.507182	-1.964032	2.861645	0.005587	0.707700
-29.760193	-1.917760	2.871642	0.005634	0.707703
-29.679934	-1.928865	2.881638	0.005619	0.707710
-28.933317	-1.910720	2.891635	0.005480	0.708013
-28.522586	-1.983649	2.901632	0.005403	0.708014
-28.785624	-1.937305	2.911629	0.005452	0.708013
-28.345923	-1.914536	2.921626	0.005370	0.708216
-27.718881	-1.959253	2.931622	0.005253	0.708351
-27.764589	-1.951101	2.941619	0.005261	0.708351
-27.676295	-1.968158	2.951616	0.005245	0.708349
-27.064341	-1.934602	2.961613	0.005130	0.708635
-26.865972	-1.966362	2.971610	0.005093	0.708643
-27.006939	-1.943924	2.981606	0.005119	0.708637
-26.717513	-1.917652	2.991603	0.005065	0.708794
-26.037829	-1.957793	3.001600	0.004939	0.708956
-26.327730	-1.905651	3.011597	0.004992	0.708957
-25.786173	-1.993732	3.021594	0.004892	0.708975
-25.314810	-1.932444	3.031590	0.004804	0.709266
-25.355263	-1.925814	3.041587	0.004811	0.709265
-25.081845	-1.973521	3.051584	0.004760	0.709267
-24.903324	-1.903267	3.061581	0.004726	0.709472
-24.239876	-1.958011	3.071578	0.004603	0.709599
-24.408089	-1.928808	3.081574	0.004634	0.709598
-24.121871	-1.969612	3.091571	0.004581	0.709618
-23.600732	-1.923816	3.101568	0.004483	0.709896
-23.277582	-1.983432	3.111565	0.004423	0.709892
-23.339616	-1.971706	3.121562	0.004434	0.709894
-23.229745	-1.898428	3.131558	0.004414	0.710080
-22.646703	-1.934518	3.141555	0.004305	0.710216
-22.445588	-1.969765	3.151552	0.004267	0.710217
-22.511549	-1.942282	3.161549	0.004280	0.710249
-21.429903	-1.992326	3.171546	0.004078	0.710534
-21.662973	-1.952076	3.181542	0.004121	0.710532
-21.543035	-1.973404	3.191539	0.004099	0.710532
-21.357094	-1.945098	3.201536	0.004064	0.710655
-20.375365	-2.010992	3.211533	0.003881	0.710873
-20.589735	-1.970944	3.221530	0.003921	0.710877
-20.733374	-1.947455	3.231526	0.003947	0.710874
-20.137831	-1.976877	3.241523	0.003836	0.711027
-19.951239	-1.954750	3.251520	0.003801	0.711138
-19.856562	-1.970518	3.261517	0.003784	0.711140
-19.851465	-1.937072	3.271514	0.003783	0.711209
-19.155451	-1.936717	3.281510	0.003653	0.711458
-18.974817	-1.970583	3.291507	0.003619	0.711455
-19.065915	-1.953834	3.301504	0.003636	0.711456
-18.219328	-1.974499	3.311501	0.003478	0.711716
-18.199198	-1.954091	3.321498	0.003474	0.711764
-18.185670	-1.957161	3.331494	0.003471	0.711763
-18.135554	-1.906498	3.341491	0.003462	0.711882
-17.297280	-1.951363	3.351488	0.003306	0.712091
-17.287831	-1.952138	3.361485	0.003304	0.712093
-17.374592	-1.930672	3.371482	0.003320	0.712105
-16.808742	-1.889884	3.381478	0.003214	0.712387
-16.502886	-1.945513	3.391475	0.003157	0.712385
-16.319854	-1.975844	3.401472	0.003123	0.712390
-16.107778	-1.904379	3.411469	0.003083	0.712608
-15.589081	-1.942392	3.421466	0.002987	0.712717
-15.772941	-1.911627	3.431462	0.003021	0.712713
-15.447353	-1.918875	3.441459	0.002960	0.712815
-14.792164	-1.929827	3.451456	0.002838	0.713025
-14.501649	-1.980011	3.461453	0.002783	0.713029
-14.435236	-1.990973	3.471450	0.002771	0.713031
-14.103190	-1.940700	3.481446	0.002709	0.713249
-13.552401	-1.983000	3.491443	0.002606	0.713360
-13.844821	-1.929871	3.501440	0.002660	0.713363
-13.793449	-1.933319	3.511437	0.002651	0.713374
-12.991743	-1.935380	3.521434	0.002501	0.713654
-12.839169	-1.962085	3.531430	0.002473	0.713656
-12.902273	-1.952250	3.541427	0.002484	0.713653
-12.666841	-1.915368	3.551424	0.002440	0.713810
-11.880077	-1.973745	3.561421	0.002294	0.713973
-12.157580	-1.924573	3.571418	0.002345	0.713973
-11.774653	-1.992435	3.581414	0.002274	0.713974
-11.219428	-1.942308	3.591411	0.002170	0.714270
-11.226946	-1.936319	3.601408	0.002171	0.714280
-10.884248	-1.994534	3.611405	0.002108	0.714286
-10.971889	-1.906000	3.621402	0.002124	0.714431
-9.838644	-2.015435	3.631398	0.001913	0.714615
-10.155335	-1.959244	3.641395	0.001971	0.714615
-9.970212	-1.993044	3.651392	0.001937	0.714613
-9.464679	-1.995465	3.661389	0.001842	0.714788
-9.273255	-1.966321	3.671386	0.001807	0.714913
-9.264973	-1.967986	3.681382	0.001805	0.714913
-9.462410	-1.918116	3.691379	0.001841	0.714943
-8.650025	-1.915829	3.701376	0.001690	0.715235
-8.371030	-1.964421	3.711373	0.001638	0.715237
-8.157804	-2.003817	3.721370	0.001598	0.715235
-7.977541	-1.942179	3.731366	0.001564	0.715421
-7.287207	-2.001104	3.741363	0.001436	0.715548
-7.587949	-1.948231	3.751360	0.001492	0.715547
-7.254769	-2.005212	3.761357	0.001429	0.715552
-6.945558	-1.907551	3.771354	0.001372	0.715855
-6.451796	-1.980831	3.781350	0.001280	0.715885
-6.505344	-1.971284	3.791347	0.001289	0.715885
-6.452985	-1.941796	3.801344	0.001279	0.715962
-5.584696	-2.008695	3.811341	0.001118	0.716136
-5.881937	-1.956251	3.821338	0.001173	0.716136
-5.680886	-1.991032	3.831334	0.001135	0.716138
-5.387957	-1.900599	3.841331	0.001080	0.716421
-4.823096	-1.985226	3.851328	0.000975	0.716453
-5.043264	-1.945329	3.861325	0.001016	0.716454
-4.611352	-1.924873	3.871322	0.000935	0.716647
-4.659679	-1.860546	3.881318	0.000944	0.716758
-4.413666	-1.905189	3.891315	0.000898	0.716757
-3.725169	-1.934659	3.901312	0.000770	0.716941
-3.392845	-1.920886	3.911309	0.000708	0.717086
-3.068945	-1.978612	3.921306	0.000647	0.717086
-3.261320	-1.933987	3.931302	0.000683	0.717107
-2.745473	-1.888153	3.941299	0.000587	0.717380
-2.987223	-1.843307	3.951296	0.000632	0.717384
-2.675417	-1.890854	3.961293	0.000573	0.717400
-2.030800	-1.848166	3.971290	0.000453	0.717711
-1.949429	-1.864312	3.981286	0.000438	0.717708
-1.693518	-1.911190	3.991283	0.000390	0.717706
-1.784448	-1.759057	4.001280	0.000407	0.717975
-1.834111	-1.726587	4.011277	0.000416	0.718022
-2.155894	-1.608459	4.021274	0.000476	0.718142
-1.781887	-1.566838	4.031270	0.000406	0.718356
-1.550361	-1.577907	4.041267	0.000363	0.718416
-1.152097	-1.531851	4.051264	0.000288	0.718648
-1.040533	-1.551713	4.061261	0.000267	0.718648
-1.226108	-1.358460	4.071258	0.000302	0.718964
-1.258411	-1.333764	4.081254	0.000307	0.719002
-0.930956	-1.255184	4.091251	0.000246	0.719272
-0.834319	-1.223006	4.101248	0.000228	0.719370
-0.857113	-1.099422	4.111245	0.000232	0.719606
-0.888219	-1.000017	4.121242	0.000238	0.719791
-0.628482	-0.977215	4.131238	0.000189	0.719928
-0.633985	-0.824833	4.141235	0.000190	0.720226
-0.698539	-0.719828	4.151232	0.000202	0.720411
-0.390492	-0.678054	4.161229	0.000144	0.720601
-0.066016	-0.592593	4.171226	0.000083	0.720883
-0.210283	-0.477199	4.181222	0.000110	0.721060
-0.479456	-0.324799	4.191219	0.000160	0.721266
-0.198289	-0.256655	4.201216	0.000107	0.721499
-0.369949	-0.093562	4.211213	0.000139	0.721759
-0.138265	0.025247	4.221210	0.000096	0.722074
0.000000	0.145206	4.231206	0.000070	0.722358

0.306618	0.737818	4.236211	0.000012	0.723628
0.638848	1.949848	4.241216	-0.000051	0.726116
1.375289	3.695362	4.246221	-0.000189	0.729772
2.420638	5.943937	4.251226	-0.000385	0.734489
3.359020	8.726515	4.256230	-0.000562	0.740163
4.449269	11.985162	4.261235	-0.000767	0.746749
6.340841	15.555735	4.266240	-0.001121	0.754133
9.209564	19.393196	4.271245	-0.001658	0.762263
13.585238	23.420785	4.276250	-0.002476	0.771149
18.947160	27.713371	4.281254	-0.003477	0.780731
23.030313	32.627780	4.286259	-0.004241	0.790903
24.308259	38.364177	4.291264	-0.004482	0.801519
25.382216	44.439013	4.296269	-0.004686	0.812524
26.261894	50.818398	4.301274	-0.004854	0.823846
26.936952	57.511600	4.306278	-0.004984	0.835485
28.093946	64.312863	4.311283	-0.005204	0.847287
28.861940	71.401703	4.316288	-0.005352	0.859287
29.699979	78.679323	4.321293	-0.005513	0.871449
30.435996	86.134442	4.326298	-0.005655	0.883699
31.366640	93.721576	4.331302	-0.005833	0.896045
33.443564	101.273632	4.336307	-0.006225	0.908480
34.233048	109.191156	4.341312	-0.006377	0.920962
34.821713	117.256249	4.346317	-0.006492	0.933447
35.704962	125.371930	4.351322	-0.006662	0.945920
36.317943	133.625699	4.356326	-0.006782	0.958364
37.343424	141.889712	4.361331	-0.006978	0.970769
38.093802	150.263246	4.366336	-0.007123	0.983105
38.844831	158.744708	4.371341	-0.007269	0.995442
39.750699	167.194302	4.376346	-0.007443	1.007620
40.823414	175.670095	4.381350	-0.007648	1.019729
41.727222	184.229280	4.386355	-0.007822	1.031769
42.462863	192.827507	4.391360	-0.007965	1.043683
43.208606	201.461699	4.396365	-0.008109	1.055514
43.984161	210.095420	4.401370	-0.008260	1.067218
44.687890	218.758995	4.406374	-0.008396	1.078819
45.497368	227.409711	4.411379	-0.008553	1.090302
46.471156	236.027549	4.416384	-0.008740	1.101659
47.117653	244.720482	4.421389	-0.008866	1.112924
47.906006	253.372825	4.426394	-0.009018	1.124055
48.726124	262.028039	4.431398	-0.009177	1.135087
49.690900	270.660003	4.436403	-0.009362	1.146015
50.163477	279.390084	4.441408	-0.009456	1.156855
51.036921	287.984936	4.446413	-0.009624	1.167514
51.895010	296.599893	4.451418	-0.009790	1.178097
52.437767	305.243785	4.456422	-0.009897	1.188555
52.899655	313.898176	4.461427	-0.009988	1.198918
53.505701	322.496339	4.466432	-0.010107	1.209155
54.165559	331.081674	4.471437	-0.010235	1.219302
54.939342	339.648101	4.476442	-0.010385	1.229365
55.538791	348.218506	4.481446	-0.010502	1.239316
56.334933	356.736595	4.486451	-0.010656	1.249167
56.839680	365.284816	4.491456	-0.010756	1.258918
57.348783	373.824369	4.496461	-0.010856	1.268585
58.273693	382.281700	4.501466	-0.011034	1.278166
58.740979	390.792025	4.506470	-0.011127	1.287648
59.227774	399.310223	4.511475	-0.011223	1.297073
59.771634	407.773414	4.516480	-0.011330	1.306381
60.444520	416.347714	4.521485	-0.011461	1.315765
61.096036	424.752061	4.526490	-0.011588	1.324897
61.617047	433.178305	4.531494	-0.011690	1.333967
62.527833	441.527018	4.536499	-0.011865	1.342961
63.128092	449.931144	4.541504	-0.011983	1.351900
63.549265	458.341556	4.546509	-0.012067	1.360755
64.127086	466.732518	4.551514	-0.012180	1.369559
64.740493	475.104023	4.556518	-0.012300	1.378293
65.461697	483.452120	4.561523	-0.012439	1.386965
65.906605	491.855181	4.566528	-0.012528	1.395593
66.500563	500.186618	4.571533	-0.012644	1.404121
67.214768	508.528113	4.576538	-0.012782	1.412627
67.677210	516.872858	4.581542	-0.012874	1.421043
68.551084	525.174524	4.586547	-0.013042	1.429434
69.256454	533.482269	4.591552	-0.013179	1.437755
69.606893	541.817158	4.596557	-0.013250	1.445996
70.056546	550.164934	4.601562	-0.013339	1.454219
70.698237	558.436566	4.606566	-0.013464	1.462353
70.990101	566.809520	4.611571	-0.013524	1.470484
71.441058	575.129048	4.616576	-0.013613	1.478543
71.929139	583.392037	4.621581	-0.013710	1.486511
72.695224	591.641934	4.626586	-0.013858	1.494467
72.976149	599.940377	4.631590	-0.013916	1.502351
73.593629	608.199823	4.636595	-0.014036	1.510209
74.142947	616.454158	4.641600	-0.014144	1.518011
74.481887	624.724878	4.646605	-0.014212	1.525756
75.258718	632.954624	4.651610	-0.014362	1.533490
75.736711	641.199478	4.656614	-0.014457	1.541154
76.038190	649.489874	4.661619	-0.014518	1.548795
76.458029	657.749630	4.666624	-0.014602	1.556388
76.876985	665.977491	4.671629	-0.014686	1.563916
77.325318	674.219499	4.676634	-0.014775	1.571424
77.833499	682.439810	4.681638	-0.014875	1.578885
78.284034	690.664518	4.686643	-0.014964	1.586307
78.681434	698.909638	4.691648	-0.015043	1.593705
78.896247	707.148243	4.696653	-0.015089	1.601036
79.351929	715.363915	4.701658	-0.015179	1.608348
79.972849	723.546523	4.706662	-0.015300	1.615621
80.215096	731.795163	4.711667	-0.015351	1.622866
80.737872	740.010793	4.716672	-0.015453	1.630088
81.061205	748.262666	4.721677	-0.015519	1.637283
81.688708	756.407346	4.726682	-0.015641	1.644395
81.987953	764.602793	4.731686	-0.015702	1.651476
82.625181	772.768496	4.736691	-0.015827	1.658546
82.875000	780.966494	4.741696	-0.015878	1.665561
83.001166	789.212171	4.746701	-0.015907	1.672571
83.424300	797.383874	4.751706	-0.015992	1.679528
83.743827	805.555208	4.756710	-0.016056	1.686443
84.027449	813.771741	4.761715	-0.016115	1.693362
84.428710	821.927703	4.766720	-0.016195	1.700218
84.847068	830.090630	4.771725	-0.016278	1.707055
85.354848	838.281179	4.776730	-0.016378	1.713898
85.597029	846.442048	4.781734	-0.016429	1.720655
85.831056	854.631044	4.786739	-0.016478	1.727408
86.382430	862.784209	4.791744	-0.016586	1.734146
86.700053	870.942179	4.796749	-0.016650	1.740832
87.015959	879.118837	4.801754	-0.016714	1.747506
87.509024	887.277173	4.806758	-0.016812	1.754163
87.877189	895.424376	4.811763	-0.016886	1.760770
88.241711	903.573518	4.816768	-0.016959	1.767353
88.663019	911.729922	4.821773	-0.017043	1.773925
89.361792	919.843626	4.826778	-0.017178	1.780472
89.362388	928.048645	4.831782	-0.017184	1.786982
89.788815	936.261884	4.836787	-0.017268	1.793527
90.349897	944.360415	4.841792	-0.017378	1.799974
90.558657	952.513369	4.846797	-0.017423	1.806397
90.843059	960.686689	4.851802	-0.017481	1.812823
91.398286	968.783300	4.856806	-0.017590	1.819199
91.822571	976.917975	4.861811	-0.017674	1.825566
92.219691	985.067070	4.866816	-0.017753	1.831919
92.676779	993.199136	4.871821	-0.017844	1.838244
92.885077	1001.360623	4.876826	-0.017888	1.844541
93.275876	1009.489365	4.881830	-0.017966	1.850812
93.723535	1017.630189	4.886835	-0.018055	1.857077
94.135263	1025.754079	4.891840	-0.018137	1.863305
94.251250	1033.932572	4.896845	-0.018164	1.869519
94.667428	1042.076478	4.901850	-0.018247	1.875720
94.861511	1050.191885	4.906854	-0.018288	1.881854
95.137304	1058.315293	4.911859	-0.018345	1.887984
95.375909	1066.461202	4.916864	-0.018395	1.894106
95.827325	1074.550469	4.921869	-0.018484	1.900190
96.402116	1082.641079	4.926874	-0.018597	1.906269
96.587125	1090.807976	4.931878	-0.018637	1.912342
97.049632	1098.916744	4.936883	-0.018728	1.918384
97.499963	1107.001748	4.941888	-0.018817	1.924387
97.769898	1115.135354	4.946893	-0.018873	1.930388
98.158356	1123.277749	4.951898	-0.018951	1.936389
98.668343	1131.356341	4.956902	-0.019051	1.942339
99.208021	1139.481071	4.961907	-0.019157	1.948306
99.658551	1147.641768	4.966912	-0.019246	1.954272
99.898065	1155.748679	4.971917	-0.019296	1.960158
100.325732	1163.841844	4.976922	-0.019381	1.966037
100.204399	1172.009643	4.981926	-0.019364	1.971892
100.615698	1180.104723	4.986931	-0.019446	1.977736
101.045451	1188.185466	4.991936	-0.019531	1.983553
101.211697	1196.312398	4.996941	-0.019567	1.989358
101.531498	1204.433809	5.001946	-0.019632	1.995159
101.680714	1212.527179	5.006950	-0.019665	2.000905
101.957863	1220.648912	5.011955	-0.019722	2.006668
102.317267	1228.746538	5.016960	-0.019795	2.012406
102.712110	1236.831175	5.021965	-0.019874	2.018122
103.301403	1244.906798	5.026970	-0.019989	2.023836
103.633930	1253.014928	5.031974	-0.020056	2.029529
104.019216	1261.150701	5.036979	-0.020133	2.035231
104.645373	1269.187952	5.041984	-0.020255	2.040874
105.090186	1277.269850	5.046989	-0.020343	2.046513
105.315523	1285.435811	5.051994	-0.020390	2.052172
105.454166	1293.546826	5.056998	-0.020422	2.057769
105.783121	1301.642434	5.062003	-0.020488	2.063360
106.024907	1309.747890	5.067008	-0.020539	2.068933
106.273594	1317.874407	5.072013	-0.020590	2.074506
106.779466	1325.927227	5.077018	-0.020690	2.080040
107.052440	1334.021510	5.082022	-0.020746	2.085564
107.613029	1342.086938	5.087027	-0.020856	2.091082
107.896289	1350.202784	5.092032	-0.020914	2.096592
108.299576	1358.279680	5.097037	-0.020994	2.102073
108.582969	1366.396960	5.102042	-0.021052	2.107555
109.082735	1374.526743	5.107046	-0.021151	2.113053
109.384404	1382.617127	5.112051	-0.021212	2.118490
109.774047	1390.673676	5.117056	-0.021290	2.123899
110.090888	1398.753797	5.122061	-0.021355	2.129303
110.690298	1406.835545	5.127066	-0.021472	2.134722
111.060323	1414.902001	5.132070	-0.021546	2.140095
111.043270	1423.038803	5.137075	-0.021548	2.145463
111.372633	1431.119122	5.142080	-0.021615	2.150814
111.681145	1439.211621	5.147085	-0.021677	2.156158
112.101287	1447.278215	5.152090	-0.021761	2.161482
112.427178	1455.343778	5.157094	-0.021827	2.166783
113.055743	1463.411693	5.162099	-0.021949	2.172101
113.534204	1471.498362	5.167104	-0.022044	2.177404
113.756399	1479.587271	5.172109	-0.022091	2.182671
114.215973	1487.673371	5.177114	-0.022182	2.187946
114.439622	1495.810789	5.182118	-0.022229	2.193220
114.606628	1503.903903	5.187123	-0.022265	2.198447
115.062137	1511.950161	5.192128	-0.022355	2.203658
115.352699	1520.027108	5.197133	-0.022415	2.208861
115.748571	1528.139790	5.202138	-0.022494	2.214085
115.804599	1536.222188	5.207142	-0.022509	2.219246
116.237038	1544.280209	5.212147	-0.022595	2.224413
116.301353	1552.405189	5.217152	-0.022613	2.229578
116.434746	1560.498699	5.222157	-0.022643	2.234717
116.813787	1568.562279	5.227162	-0.022719	2.239847
117.071108	1576.600156	5.232166	-0.022772	2.244939
117.279592	1584.702777	5.237171	-0.022816	2.250055
117.512845	1592.805866	5.242176	-0.022865	2.255162
118.112667	1600.848616	5.247181	-0.022982	2.260251
118.371264	1608.922522	5.252186	-0.023035	2.265319
118.452992	1617.035202	5.257190	-0.023056	2.270384
119.014613	1625.142621	5.262195	-0.023166	2.275476
119.431221	1633.154204	5.267200	-0.023249	2.280485
119.534997	1641.217533	5.272205	-0.023273	2.285488
119.827317	1649.300956	5.277210	-0.023333	2.290508
120.108952	1657.357171	5.282214	-0.023391	2.295500
120.300513	1665.433345	5.287219	-0.023432	2.300485
120.312868	1673.527082	5.292224	-0.023440	2.305455
120.629156	1681.578045	5.297229	-0.023504	2.310414
121.105404	1689.642033	5.302234	-0.023598	2.315384
121.400782	1697.682813	5.307238	-0.023658	2.320313
121.516931	1705.762789	5.312243	-0.023685	2.325241
122.001390	1713.816258	5.317248	-0.023781	2.330173
122.267398	1721.906018	5.322253	-0.023836	2.335098
122.880773	1729.931248	5.327258	-0.023955	2.340002
122.832035	1738.017205	5.332262	-0.023951	2.344879
123.165452	1746.106870	5.337267	-0.024019	2.349779
123.484053	1754.219043	5.342272	-0.024084	2.354680
123.803260	1762.255517	5.347277	-0.024148	2.359526
124.124280	1770.298051	5.352282	-0.024213	2.364366
124.384586	1778.362850	5.357286	-0.024267	2.369205
124.632470	1786.462506	5.362291	-0.024319	2.374053
125.171893	1794.497201	5.367296	-0.024424	2.378876
125.401796	1802.539533	5.372301	-0.024473	2.383668
125.857983	1810.601680	5.377306	-0.024563	2.388481
126.317768	1818.657459	5.382310	-0.024654	2.393281
126.718544	1826.723832	5.387315	-0.024734	2.398072
126.561167	1834.830592	5.392320	-0.024710	2.402834
126.909166	1842.878374	5.397325	-0.024780	2.407592
127.062269	1850.998846	5.402330	-0.024814	2.412367
127.274433	1859.056953	5.407334	-0.024859	2.417101
127.502974	1867.102895	5.412339	-0.024907	2.421820
127.919438	1875.144381	5.417344	-0.024989	2.426541
128.086315	1883.262974	5.422349	-0.025026	2.431279
128.323914	1891.370709	5.427354	-0.025075	2.436006
128.816573	1899.345677	5.432358	-0.025172	2.440667
129.124796	1907.399090	5.437363	-0.025235	2.445351
129.235741	1915.472684	5.442368	-0.025261	2.450022
129.493140	1923.533347	5.447373	-0.025314	2.454687
129.734375	1931.601317	5.452378	-0.025365	2.459347
130.127074	1939.609986	5.457382	-0.025443	2.463975
130.528837	1947.675047	5.462387	-0.025523	2.468628
131.016626	1955.727715	5.467392	-0.025619	2.473271
131.209508	1963.804390	5.472397	-0.025661	2.477896
131.331529	1971.868487	5.477402	-0.025689	2.482501
131.426030	1979.916882	5.482406	-0.025712	2.487087
131.677802	1987.994770	5.487411	-0.025764	2.491692
131.700701	1996.092570	5.492416	-0.025773	2.496283
132.003047	2004.114794	5.497421	-0.025835	2.500843
132.438853	2012.157889	5.502426	-0.025922	2.505416
132.656497	2020.233250	5.507430	-0.025967	2.509984
132.924798	2028.322784	5.512435	-0.026023	2.514554
133.276740	2036.355546	5.517440	-0.026094	2.519091
133.485090	2044.369303	5.522445	-0.026138	2.523598
133.663367	2052.445772	5.527450	-0.026176	2.528130
133.909190	2060.509200	5.532454	-0.026227	2.532652
134.255323	2068.565993	5.537459	-0.026297	2.537168
134.448894	2076.614417	5.542464	-0.026338	2.541662
134.555341	2084.662986	5.547469	-0.026364	2.546141
134.978313	2092.735178	5.552474	-0.026448	2.550647
135.163994	2100.799521	5.557478	-0.026488	2.555125
135.216118	2108.863382	5.562483	-0.026503	2.559585
135.456405	2116.884141	5.567488	-0.026553	2.564027
135.614561	2124.938411	5.572493	-0.026587	2.568473
135.866316	2133.013703	5.577498	-0.026640	2.572930
136.086548	2141.049622	5.582502	-0.026686	2.577356
136.628905	2149.076985	5.587507	-0.026792	2.581791
136.932979	2157.144386	5.592512	-0.026854	2.586224
137.066397	2165.245484	5.597517	-0.026884	2.590656
137.437023	2173.460446	5.602522	-0.026959	2.595159
137.620902	2181.414599	5.607526	-0.026998	2.599499
137.771303	2189.427756	5.612531	-0.027032	2.603862
138.072195	2197.438886	5.617536	-0.027093	2.608227
138.257003	2205.498255	5.622541	-0.027133	2.612602
138.502111	2213.530238	5.627546	-0.027184	2.616960
138.798887	2221.545618	5.632550	-0.027244	2.621304
139.293410	2229.571773	5.637555	-0.027342	2.625660
139.513177	2237.639396	5.642560	-0.027388	2.630013
139.626593	2245.729274	5.647565	-0.027414	2.634364
139.797426	2253.776855	5.652570	-0.027452	2.638689
140.246380	2261.764730	5.657574	-0.027540	2.642993
140.461821	2269.818538	5.662579	-0.027586	2.647309
140.988754	2277.862692	5.667584	-0.027689	2.651634
141.523252	2285.897370	5.672589	-0.027794	2.655947
141.963692	2293.959860	5.677594	-0.027881	2.660262
142.117191	2302.001229	5.682598	-0.027915	2.664539
142.456757	2310.063039	5.687603	-0.027984	2.668833
142.654585	2318.178895	5.692608	-0.028026	2.673139
142.792903	2326.208701	5.697613	-0.028057	2.677389
143.047696	2334.257980	5.702618	-0.028110	2.681650
143.027162	2342.294772	5.707622	-0.028111	2.685880
143.195633	2350.343397	5.712627	-0.028148	2.690122
143.702375	2358.389048	5.717632	-0.028248	2.694376
143.788449	2366.420247	5.722637	-0.028269	2.698590
144.239841	2374.463748	5.727642	-0.028359	2.702827
144.251791	2382.516044	5.732646	-0.028366	2.707034
144.418804	2390.577283	5.737651	-0.028403	2.711248
144.653106	2398.657523	5.742656	-0.028451	2.715470
144.785894	2406.654434	5.747661	-0.028481	2.719636
145.137790	2414.696554	5.752666	-0.028552	2.723833
145.292554	2422.731950	5.757670	-0.028586	2.728007
145.499426	2430.812198	5.762675	-0.028630	2.732202
145.916210	2438.852276	5.767680	-0.028713	2.736382
146.339581	2446.851429	5.772685	-0.028797	2.740535
146.679882	2454.909177	5.777690	-0.028866	2.744706
146.824042	2462.976419	5.782694	-0.028898	2.748865
147.183677	2471.082895	5.787699	-0.028971	2.753050
147.527550	2479.108116	5.792704	-0.029040	2.757186
147.609005	2487.148952	5.797709	-0.029060	2.761308
147.835563	2495.173844	5.802714	-0.029108	2.765424
148.101345	2503.193384	5.807718	-0.029163	2.769534
148.412504	2511.268727	5.812723	-0.029226	2.773669
148.469889	2519.319001	5.817728	-0.029242	2.777769
148.715372	2527.326107	5.822733	-0.029293	2.781853
149.096469	2535.371221	5.827738	-0.029369	2.785958
149.164933	2543.407373	5.832742	-0.029387	2.790034
149.453321	2551.484175	5.837747	-0.029446	2.794138
149.607891	2559.514915	5.842752	-0.029480	2.798204
149.775885	2567.524296	5.847757	-0.029517	2.802255
150.170301	2575.566394	5.852762	-0.029596	2.806329
150.378165	2583.591573	5.857766	-0.029640	2.810378
150.658229	2591.651251	5.862771	-0.029697	2.814443
150.606651	2599.747710	5.867776	-0.029693	2.818501
150.619995	2607.776021	5.872781	-0.029701	2.822522
151.058792	2615.810260	5.877786	-0.029788	2.826566
151.183209	2623.874620	5.882790	-0.029816	2.830600
151.583806	2631.920974	5.887795	-0.029896	2.834636
151.816561	2639.941651	5.892800	-0.029945	2.838643
151.740634	2647.969898	5.897805	-0.029936	2.842631
152.030941	2656.003731	5.902810	-0.029995	2.846637
152.284271	2664.029292	5.907814	-0.030048	2.850631
152.470145	2672.106053	5.912819	-0.030088	2.854641
152.579681	2680.144130	5.917824	-0.030114	2.858622
152.879646	2688.146736	5.922829	-0.030175	2.862590
153.244811	2696.203976	5.927834	-0.030248	2.866583
153.353318	2704.240545	5.932838	-0.030274	2.870547
153.578526	2712.295549	5.937843	-0.030321	2.874520
153.959654	2720.331674	5.942848	-0.030397	2.878487
153.948215	2728.363661	5.947853	-0.030400	2.882425
154.396255	2736.395639	5.952858	-0.030489	2.886383
154.683891	2744.417760	5.957862	-0.030548	2.890322
154.793796	2752.496307	5.962867	-0.030574	2.894273
154.891621	2760.549505	5.967872	-0.030597	2.898206
155.079104	2768.581974	5.972877	-0.030637	2.902128
155.359526	2776.621579	5.977882	-0.030695	2.906053
155.424915	2784.668259	5.982886	-0.030713	2.909965
155.808736	2792.769348	5.987891	-0.030789	2.913915
156.358863	2800.758895	5.992896	-0.030897	2.917815
156.404425	2808.766320	5.997901	-0.030911	2.921691
156.578523	2816.798148	6.002906	-0.030949	2.925580
156.854659	2824.801126	6.007910	-0.031005	2.929456
157.277982	2832.859106	6.012915	-0.031089	2.933360
157.400415	2840.906276	6.017920	-0.031118	2.937239
157.583327	2848.919876	6.022925	-0.031157	2.941099
157.897023	2856.985256	6.027930	-0.031221	2.944986
157.971944	2865.010403	6.032934	-0.031240	2.948836
158.037898	2873.086218	6.037939	-0.031258	2.952705
158.274450	2881.130079	6.042944	-0.031307	2.956562
158.401237	2889.130958	6.047949	-0.031336	2.960388
158.605646	2897.162749	6.052954	-0.031379	2.964228
158.806526	2905.196263	6.057958	-0.031422	2.968063
159.003849	2913.257744	6.062963	-0.031464	2.971907
159.282903	2921.306563	6.067968	-0.031521	2.975743
159.397939	2929.311634	6.072973	-0.031548	2.979546
159.896248	2937.337612	6.077978	-0.031646	2.983373
159.940931	2945.397968	6.082982	-0.031660	2.987188
160.297798	2953.430897	6.087987	-0.031731	2.991002
160.763317	2961.472694	6.092992	-0.031823	2.994819
160.826338	2969.491996	6.097997	-0.031841	2.998602
161.046532	2977.531423	6.103002	-0.031887	3.002397
161.296298	2985.546129	6.108006	-0.031939	3.006176
161.529246	2993.571497	6.113011	-0.031987	3.009956
161.920294	3001.647785	6.118016	-0.032065	3.013762
161.904309	3009.672403	6.123021	-0.032068	3.017519
162.200196	3017.721163	6.128026	-0.032128	3.021297
162.259908	3025.735261	6.133030	-0.032145	3.025044
162.324762	3033.784911	6.138035	-0.032162	3.028802
162.574419	3041.845496	6.143040	-0.032214	3.032570
162.630891	3049.879909	6.148045	-0.032230	3.036312
162.881677	3057.898760	6.153050	-0.032282	3.040051
163.344453	3065.893587	6.158054	-0.032373	3.043785
163.578684	3073.941605	6.163059	-0.032422	3.047528
163.748248	3082.015077	6.168064	-0.032459	3.051274
164.018006	3090.040309	6.173069	-0.032515	3.054999
164.405394	3098.076935	6.178074	-0.032592	3.058730
164.750837	3106.091314	6.183078	-0.032662	3.062444
164.871004	3114.131181	6.188083	-0.032689	3.066154
165.444828	3122.157642	6.193088	-0.032801	3.069875
165.811397	3130.262824	6.198093	-0.032875	3.073618
166.126460	3138.281937	6.203098	-0.032939	3.077315
166.353958	3146.296582	6.208102	-0.032987	3.081000
166.559376	3154.279534	6.213107	-0.033030	3.084666
166.703062	3162.343887	6.218112	-0.033062	3.088362
166.738738	3170.391273	6.223117	-0.033074	3.092041
166.970287	3178.464828	6.228122	-0.033123	3.095736
167.087032	3186.464431	6.233126	-0.033150	3.099388
167.296203	3194.456718	6.238131	-0.033194	3.103036
167.549812	3202.511093	6.243136	-0.033247	3.106710
167.671114	3210.529898	6.248141	-0.033274	3.110358
167.953979	3218.590277	6.253146	-0.033332	3.114028
167.996348	3226.638056	6.258150	-0.033346	3.117677
168.338537	3234.631698	6.263155	-0.033415	3.121310
168.726288	3242.620644	6.268160	-0.033492	3.124939
168.630966	3250.692463	6.273165	-0.033480	3.128579
169.101378	3258.724716	6.278170	-0.033573	3.132223
169.294337	3266.794599	6.283174	-0.033614	3.135867
169.403204	3274.795463	6.288179	-0.033639	3.139472
169.630715	3282.858580	6.293184	-0.033687	3.143106
169.784507	3290.861133	6.298189	-0.033721	3.146706
170.008015	3298.919063	6.303194	-0.033768	3.150329
170.026527	3306.960356	6.308198	-0.033777	3.153931
170.424393	3314.959961	6.313203	-0.033856	3.157527
170.547376	3323.022164	6.318208	-0.033884	3.161135
170.784857	3330.995066	6.323213	-0.033934	3.164704
171.153505	3339.030258	6.328218	-0.034008	3.168303
171.496144	3347.056246	6.333222	-0.034077	3.171892
171.661147	3355.119159	6.338227	-0.034113	3.175486
171.911876	3363.150709	6.343232	-0.034165	3.179065
172.129951	3371.155164	6.348237	-0.034211	3.182627
172.194457	3379.240488	6.353242	-0.034228	3.186214
172.318435	3387.269318	6.358246	-0.034257	3.189775
172.526392	3395.316829	6.363251	-0.034301	3.193343
172.851821	3403.349542	6.368256	-0.034367	3.196906
172.761228	3411.365092	6.373261	-0.034355	3.200440
172.979376	3419.386403	6.378266	-0.034401	3.203985
173.243829	3427.385375	6.383270	-0.034456	3.207519
173.576138	3435.417435	6.388275	-0.034523	3.211066
173.471038	3443.528207	6.393280	-0.034509	3.214625
173.570758	3451.519056	6.398285	-0.034532	3.218136
174.011272	3459.534441	6.403290	-0.034620	3.221669
174.264261	3467.526480	6.408294	-0.034672	3.225179
174.614076	3475.553297	6.413299	-0.034743	3.228705
175.022273	3483.628660	6.418304	-0.034824	3.232250
175.053530	3491.688781	6.423309	-0.034835	3.235769
175.309887	3499.688077	6.428314	-0.034888	3.239268
175.462172	3507.694323	6.433318	-0.034922	3.242761
175.601215	3515.737792	6.438323	-0.034953	3.246266
175.915000	3523.755214	6.443328	-0.035017	3.249763
176.282858	3531.754146	6.448333	-0.035090	3.253250
176.616392	3539.813985	6.453338	-0.035158	3.256759
176.657333	3547.861926	6.458342	-0.035171	3.260247
176.691516	3555.879429	6.463347	-0.035183	3.263717
177.073805	3563.913447	6.468352	-0.035259	3.267205
177.023350	3571.947208	6.473357	-0.035255	3.270672
177.404936	3579.983503	6.478362	-0.035331	3.274153
177.914223	3587.998109	6.483366	-0.035431	3.277627
178.192615	3596.022781	6.488371	-0.035489	3.281091
178.390942	3604.044423	6.493376	-0.035531	3.284548
178.624600	3612.072887	6.498381	-0.035580	3.288005
178.830575	3620.129158	6.503386	-0.035623	3.291470
178.950936	3628.173284	6.508390	-0.035651	3.294922
179.009001	3636.175315	6.513395	-0.035667	3.298351
179.317052	3644.202803	6.518400	-0.035730	3.301796
179.487371	3652.206516	6.523405	-0.035767	3.305222
179.611607	3660.273955	6.528410	-0.035795	3.308670
179.890775	3668.309012	6.533414	-0.035853	3.312106
180.110739	3676.357802	6.538419	-0.035899	3.315542
180.387826	3684.358614	6.543424	-0.035956	3.318957
180.500394	3692.353655	6.548429	-0.035982	3.322359
180.872464	3700.369427	6.553434	-0.036057	3.325777
180.946576	3708.419793	6.558438	-0.036076	3.329194
181.042353	3716.474364	6.563443	-0.036099	3.332610
181.168313	3724.531663	6.568448	-0.036128	3.336026
181.392567	3732.503760	6.573453	-0.036175	3.339405
181.780925	3740.517830	6.578458	-0.036252	3.342804
181.797115	3748.556283	6.583462	-0.036261	3.346197
182.041150	3756.561680	6.588467	-0.036311	3.349581
182.476473	3764.660377	6.593472	-0.036398	3.353007
182.552525	3772.687930	6.598477	-0.036417	3.356387
182.755028	3780.714223	6.603482	-0.036460	3.359768
182.848350	3788.703022	6.608486	-0.036483	3.363125
183.197011	3796.730112	6.613491	-0.036553	3.366504
183.559183	3804.762796	6.618496	-0.036626	3.369883
183.446482	3812.837500	6.623501	-0.036610	3.373259
183.734916	3820.882383	6.628506	-0.036669	3.376633
183.953874	3828.877796	6.633510	-0.036715	3.379981
184.072847	3836.884475	6.638515	-0.036743	3.383326
184.296401	3844.936759	6.643520	-0.036790	3.386691
184.365327	3852.938201	6.648525	-0.036808	3.390026
184.703468	3861.066806	6.653530	-0.036876	3.393420
184.845570	3869.070623	6.658534	-0.036908	3.396752
185.020149	3877.039786	6.663539	-0.036946	3.400067
185.298911	3885.060068	6.668544	-0.037003	3.403404
185.367465	3893.077989	6.673549	-0.037021	3.406729
185.586531	3901.079954	6.678554	-0.037067	3.410050
185.896769	3909.115495	6.683558	-0.037130	3.413384
185.975792	3917.177422	6.688563	-0.037150	3.416718
186.078866	3925.183237	6.693568	-0.037175	3.420026
186.414358	3933.177719	6.698573	-0.037242	3.423335
186.679832	3941.236646	6.703578	-0.037297	3.426664
186.756806	3949.259042	6.708582	-0.037317	3.429969
186.851403	3957.295374	6.713587	-0.037340	3.433276
187.103470	3965.341107	6.718592	-0.037392	3.436590
187.083941	3973.345294	6.723597	-0.037394	3.439874
187.354047	3981.345803	6.728602	-0.037449	3.443164
187.509998	3989.401468	6.733606	-0.037484	3.446469
187.712470	3997.395545	6.738611	-0.037527	3.449747
188.086431	4005.488174	6.743616	-0.037602	3.453068
188.212943	4013.515374	6.748621	-0.037631	3.456350
188.465900	4021.520227	6.753626	-0.037683	3.459625
188.892570	4029.531148	6.758630	-0.037768	3.462905
188.895314	4037.571438	6.763635	-0.037773	3.466179
189.055617	4045.607561	6.768640	-0.037809	3.469454
189.338772	4053.656200	6.773645	-0.037867	3.472735
189.404045	4061.720624	6.778650	-0.037884	3.476012
189.617808	4069.666253	6.783654	-0.037929	3.479243
189.729179	4077.662892	6.788659	-0.037955	3.482488
189.856736	4085.702025	6.793664	-0.037984	3.485748
189.980569	4093.715846	6.798669	-0.038013	3.488994
190.427225	4101.750565	6.803674	-0.038101	3.492256
190.443426	4109.838218	6.808678	-0.038110	3.495523
190.551877	4117.796979	6.813683	-0.038135	3.498737
191.015923	4125.810657	6.818688	-0.038227	3.501982
191.700811	4133.782302	6.823693	-0.038360	3.505213
191.806757	4141.850624	6.828698	-0.038385	3.508463
192.138171	4149.891228	6.833702	-0.038452	3.511705
192.488062	4157.918557	6.838707	-0.038522	3.514939
192.660919	4165.956907	6.843712	-0.038560	3.518170
192.922886	4173.962407	6.848717	-0.038614	3.521386
193.052088	4181.980806	6.853722	-0.038643	3.524601
193.351357	4190.010042	6.858726	-0.038704	3.527823
193.405329	4198.062261	6.863731	-0.038719	3.531043
193.502212	4206.130344	6.868736	-0.038743	3.534268
193.758791	4214.144469	6.873741	-0.038796	3.537474
193.790390	4222.174318	6.878746	-0.038807	3.540676
193.931047	4230.156992	6.883750	-0.038839	3.543859
194.165586	4238.199535	6.888755	-0.038888	3.547066
194.555782	4246.253550	6.893760	-0.038966	3.550280
194.544521	4254.365426	6.898765	-0.038969	3.553502
194.813210	4262.374118	6.903770	-0.039024	3.556688
195.017824	4270.317669	6.908774	-0.039067	3.559843
195.012475	4278.331209	6.913779	-0.039072	3.563017
195.421532	4286.348158	6.918784	-0.039153	3.566202
195.476152	4294.342464	6.923789	-0.039169	3.569364
195.628863	4302.418128	6.928794	-0.039202	3.572559
195.806323	4310.424901	6.933798	-0.039241	3.575725
195.924595	4318.414663	6.938803	-0.039268	3.578879
196.267232	4326.456240	6.943808	-0.039337	3.582057
196.332178	4334.483233	6.948813	-0.039355	3.585219
196.479002	4342.515389	6.953818	-0.039387	3.588382
196.661189	4350.548973	6.958822	-0.039427	3.591544
196.953087	4358.565913	6.963827	-0.039486	3.594699
197.120741	4366.586223	6.968832	-0.039523	3.597850
197.180650	4374.592673	6.973837	-0.039539	3.600990
197.369406	4382.557056	6.978842	-0.039580	3.604114
197.533664	4390.630780	6.983846	-0.039615	3.607277
197.718407	4398.626315	6.988851	-0.039655	3.610407
198.104549	4406.700983	6.993856	-0.039732	3.613571
198.218873	4414.722072	6.998861	-0.039759	3.616704
198.522880	4422.703960	7.003866	-0.039821	3.619824
198.809485	4430.739807	7.008870	-0.039880	3.622962
198.828299	4438.784671	7.013875	-0.039888	3.626094
198.873315	4446.821019	7.018880	-0.039902	3.629220
199.062375	4454.874383	7.023885	-0.039943	3.632354
199.336953	4462.907125	7.028890	-0.039999	3.635479
199.254109	4470.916918	7.033894	-0.039989	3.638583
199.542173	4478.910306	7.038899	-0.040048	3.641688
199.865879	4486.934012	7.043904	-0.040113	3.644804
199.982917	4494.950677	7.048909	-0.040141	3.647908
199.998400	4503.007856	7.053914	-0.040149	3.651022
200.560097	4511.022476	7.058918	-0.040259	3.654132
200.713434	4519.050149	7.063923	-0.040293	3.657234
200.621229	4527.099773	7.068928	-0.040281	3.660334
200.861066	4535.076934	7.073933	-0.040331	3.663413
201.065190	4543.107968	7.078938	-0.040374	3.666509
201.415219	4551.148245	7.083942	-0.040444	3.669610
201.838554	4559.153982	7.088947	-0.040529	3.672697
202.403499	4567.217377	7.093952	-0.040639	3.675807
202.502487	4575.192749	7.098957	-0.040663	3.678868
202.555540	4583.219439	7.103962	-0.040678	3.681945
202.710514	4591.213482	7.108966	-0.040712	3.685010
202.944643	4599.231060	7.113971	-0.040761	3.688084
203.042818	4607.319151	7.118976	-0.040785	3.691178
203.208337	4615.339323	7.123981	-0.040821	3.694245
203.482249	4623.364042	7.128986	-0.040877	3.697314
203.447201	4631.363341	7.133990	-0.040876	3.700364
203.419896	4639.354788	7.138995	-0.040876	3.703408
204.072979	4647.401283	7.144000	-0.041003	3.706487
204.077911	4655.415486	7.149005	-0.041009	3.709535
204.182915	4663.535840	7.154010	-0.041034	3.712624
204.512762	4671.571207	7.159014	-0.041101	3.715683
204.878024	4679.488415	7.164019	-0.041174	3.718696
204.985530	4687.522642	7.169024	-0.041199	3.721744
204.863521	4695.517146	7.174029	-0.041182	3.724769
205.176148	4703.554805	7.179034	-0.041246	3.727819
205.229656	4711.590032	7.184038	-0.041261	3.730859
205.311386	4719.623444	7.189043	-0.041281	3.733896
205.683056	4727.626128	7.194048	-0.041356	3.736926
205.706999	4735.627536	7.199053	-0.041366	3.739945
205.845548	4743.651445	7.204058	-0.041397	3.742973
206.077383	4751.706773	7.209062	-0.041445	3.746012
206.282987	4759.696520	7.214067	-0.041489	3.749024
206.479767	4767.774739	7.219072	-0.041531	3.752066
206.592332	4775.778364	7.224077	-0.041557	3.755076
206.780030	4783.782999	7.229082	-0.041597	3.758085
206.950591	4791.863472	7.234086	-0.041634	3.761120
206.755108	4799.802166	7.239091	-0.041603	3.764091
207.090960	4807.854686	7.244096	-0.041671	3.767114
207.215021	4815.878324	7.249101	-0.041699	3.770119
207.342934	4823.920721	7.254106	-0.041729	3.773129
207.546730	4831.981731	7.259110	-0.041772	3.776145
207.761549	4839.932319	7.264115	-0.041817	3.779118
207.973429	4847.989088	7.269120	-0.041862	3.782128
207.810037	4856.017890	7.274125	-0.041837	3.785117
208.230702	4864.023102	7.279130	-0.041920	3.788107
208.433786	4872.093116	7.284134	-0.041964	3.791115
208.193403	4880.112803	7.289139	-0.041924	3.794091
208.442351	4888.129068	7.294144	-0.041976	3.797075
208.570815	4896.084824	7.299149	-0.042005	3.800031
208.851424	4904.108620	7.304154	-0.042063	3.803014
208.808251	4912.150233	7.309158	-0.042060	3.805993
209.066508	4920.115597	7.314163	-0.042113	3.808949
209.165794	4928.207925	7.319168	-0.042137	3.811946
209.256817	4936.194814	7.324173	-0.042159	3.814901
209.482450	4944.218198	7.329178	-0.042207	3.817870
209.873926	4952.235841	7.334182	-0.042285	3.820839
209.872925	4960.230790	7.339187	-0.042290	3.823788
210.194113	4968.307527	7.344192	-0.042355	3.826772
210.409323	4976.273809	7.349197	-0.042400	3.829711
210.460129	4984.347303	7.354202	-0.042415	3.832683
210.738782	4992.346247	7.359206	-0.042472	3.835631
211.134257	5000.336377	7.364211	-0.042551	3.838575
211.373321	5008.396057	7.369216	-0.042601	3.841539
211.191360	5016.378421	7.374221	-0.042572	3.844464
211.329935	5024.443445	7.379226	-0.042604	3.847424
211.644339	5032.459772	7.384230	-0.042667	3.850367
211.629582	5040.492958	7.389235	-0.042670	3.853307
212.045186	5048.555452	7.394240	-0.042753	3.856265
212.187785	5056.511184	7.399245	-0.042785	3.859176
212.374958	5064.523564	7.404250	-0.042825	3.862106
212.511366	5072.563721	7.409254	-0.042855	3.865042
212.785784	5080.627376	7.414259	-0.042912	3.867988
212.696142	5088.693076	7.419264	-0.042901	3.870926
212.844173	5096.908128	7.424269	-0.042934	3.873920
213.310551	5104.872935	7.429274	-0.043026	3.876826
213.560135	5112.771382	7.434278	-0.043077	3.879703
213.478792	5120.733925	7.439283	-0.043067	3.882594
213.606261	5128.708445	7.444288	-0.043096	3.885491
213.679328	5136.769364	7.449293	-0.043115	3.888416
213.832483	5144.800268	7.454298	-0.043149	3.891330
213.931255	5152.815127	7.459302	-0.043173	3.894235
214.163533	5160.829865	7.464307	-0.043221	3.897140
214.462715	5168.831643	7.469312	-0.043282	3.900039
214.308396	5176.843290	7.474317	-0.043259	3.902931
214.717785	5184.840172	7.479322	-0.043341	3.905827
214.907596	5192.862330	7.484326	-0.043381	3.908725
215.081162	5200.885305	7.489331	-0.043419	3.911621
215.247890	5208.960603	7.494336	-0.043455	3.914533
215.367518	5216.922086	7.499341	-0.043483	3.917402
215.637696	5224.932138	7.504346	-0.043538	3.920288
215.547264	5232.969143	7.509350	-0.043527	3.923176
215.551593	5240.975943	7.514355	-0.043533	3.926052
215.862219	5248.994063	7.519360	-0.043596	3.928936
215.756937	5257.052162	7.524365	-0.043582	3.931825
216.017283	5265.056904	7.529370	-0.043636	3.934698
216.347257	5273.071123	7.534374	-0.043702	3.937575
216.484201	5281.070389	7.539379	-0.043733	3.940440
216.754735	5289.075924	7.544384	-0.043789	3.943308
216.922341	5297.124814	7.549389	-0.043825	3.946187
217.224527	5305.129331	7.554394	-0.043887	3.949051
217.293957	5313.203679	7.559398	-0.043905	3.951934
217.288288	5321.237692	7.564403	-0.043909	3.954798
217.659800	5329.247859	7.569408	-0.043984	3.957659
217.764839	5337.208435	7.574413	-0.044009	3.960496
218.007823	5345.226068	7.579418	-0.044059	3.963352
218.085968	5353.288234	7.584422	-0.044079	3.966220
218.233351	5361.246613	7.589427	-0.044112	3.969050
218.431108	5369.334138	7.594432	-0.044154	3.971925
218.603152	5377.342562	7.599437	-0.044191	3.974769
218.786468	5385.349224	7.604442	-0.044231	3.977611
218.817022	5393.400599	7.609446	-0.044242	3.980464
218.818976	5401.367358	7.614451	-0.044247	3.983284
219.163831	5409.411218	7.619456	-0.044317	3.986136
219.217739	5417.459452	7.624461	-0.044332	3.988982
219.287836	5425.493267	7.629466	-0.044351	3.991821
219.656161	5433.530640	7.634470	-0.044425	3.994664
219.809054	5441.524438	7.639475	-0.044458	3.997486
220.018683	5449.535548	7.644480	-0.044503	4.000314
220.343196	5457.523272	7.649485	-0.044568	4.003132
220.698127	5465.555323	7.654490	-0.044640	4.005965
220.701188	5473.579738	7.659494	-0.044646	4.008788
220.723326	5481.595636	7.664499	-0.044655	4.011606
221.000142	5489.647624	7.669504	-0.044712	4.014438
221.210815	5497.645185	7.674509	-0.044756	4.017249
221.252194	5505.695100	7.679514	-0.044769	4.020073
221.346098	5513.708294	7.684518	-0.044792	4.022883
221.337495	5521.689719	7.689523	-0.044796	4.025679
221.535905	5529.732806	7.694528	-0.044838	4.028497
221.638681	5537.778624	7.699533	-0.044863	4.031313
221.822317	5545.888278	7.704538	-0.044902	4.034150
221.869317	5553.881738	7.709542	-0.044916	4.036942
222.157049	5561.801553	7.714547	-0.044975	4.039711
222.511609	5569.819887	7.719552	-0.045046	4.042513
222.590793	5577.817097	7.724557	-0.045066	4.045302
222.674339	5585.810714	7.729562	-0.045087	4.048087
222.906623	5593.876305	7.734566	-0.045136	4.050898
223.029723	5601.886625	7.739571	-0.045164	4.053686
223.288424	5609.957072	7.744576	-0.045218	4.056495
223.190698	5617.899646	7.749581	-0.045205	4.059252
223.456858	5625.919848	7.754586	-0.045260	4.062040
223.732918	5633.933565	7.759590	-0.045316	4.064823
223.802968	5641.943300	7.764595	-0.045335	4.067601
224.068951	5650.006476	7.769600	-0.045389	4.070397
224.164157	5658.014561	7.774605	-0.045412	4.073170
224.105355	5666.064152	7.779610	-0.045407	4.075954
224.300064	5674.056661	7.784614	-0.045448	4.078720
224.438085	5682.077739	7.789619	-0.045479	4.081492
224.671629	5690.045354	7.794624	-0.045528	4.084246
224.978132	5698.096143	7.799629	-0.045591	4.087027
225.407759	5706.096977	7.804634	-0.045676	4.089791
225.419386	5714.174159	7.809638	-0.045683	4.092574
225.389998	5722.173170	7.814643	-0.045683	4.095327
225.713059	5730.193865	7.819648	-0.045749	4.098091
225.910810	5738.193151	7.824653	-0.045791	4.100843
225.987562	5746.204358	7.829658	-0.045810	4.103597
226.226234	5754.248465	7.834662	-0.045860	4.106361
226.332223	5762.252161	7.839667	-0.045885	4.109109
226.551462	5770.339880	7.844672	-0.045931	4.111885
226.600949	5778.341097	7.849677	-0.045946	4.114627
226.710976	5786.366395	7.854682	-0.045972	4.117376
226.796350	5794.324096	7.859686	-0.045993	4.120100
227.042497	5802.328652	7.864691	-0.046044	4.122840
227.426129	5810.349123	7.869696	-0.046121	4.125585
227.467262	5818.364772	7.874701	-0.046134	4.128323
227.726130	5826.409872	7.879706	-0.046187	4.131072
227.858873	5834.494317	7.884710	-0.046217	4.133830
228.002955	5842.490343	7.889715	-0.046249	4.136557
228.178926	5850.507076	7.894720	-0.046287	4.139290
228.361403	5858.536295	7.899725	-0.046327	4.142024
228.481812	5866.506990	7.904730	-0.046354	4.144737
228.683560	5874.569225	7.909734	-0.046397	4.147479
228.660539	5882.590516	7.914739	-0.046398	4.150204
228.858558	5890.655376	7.919744	-0.046440	4.152944
228.864567	5898.623665	7.924749	-0.046447	4.155647
229.044156	5906.594857	7.929754	-0.046486	4.158351
229.273272	5914.659966	7.934758	-0.046534	4.161086
229.478837	5922.612285	7.939763	-0.046577	4.163780
229.684537	5930.690767	7.944768	-0.046621	4.166516
229.704003	5938.676544	7.949773	-0.046630	4.169216
229.999233	5946.722058	7.954778	-0.046690	4.171938
230.218875	5954.746798	7.959782	-0.046736	4.174650
229.986157	5962.777015	7.964787	-0.046698	4.177357
230.287273	5970.757748	7.969792	-0.046759	4.180052
230.481492	5978.748184	7.974797	-0.046801	4.182747
230.628109	5986.776009	7.979802	-0.046834	4.185452
230.727604	5994.831033	7.984806	-0.046857	4.188164
231.031136	6002.855060	7.989811	-0.046919	4.190866
231.253556	6011.014280	7.994816	-0.046966	4.193611
231.341231	6018.950784	7.999821	-0.046988	4.196278
231.519067	6026.898839	8.004826	-0.047026	4.198948
231.513642	6034.930389	8.009830	-0.047030	4.201642
231.549814	6042.851225	8.014835	-0.047042	4.204298
231.745244	6050.922235	8.019840	-0.047084	4.207004
231.907199	6058.909085	8.024845	-0.047119	4.209680
232.113348	6066.964138	8.029850	-0.047163	4.212377
232.372109	6074.994832	8.034854	-0.047217	4.215065
232.321623	6082.973744	8.039859	-0.047212	4.217731
232.369571	6091.003367	8.044864	-0.047227	4.220413
232.495422	6098.983404	8.049869	-0.047255	4.223078
232.603334	6107.014014	8.054874	-0.047281	4.225757
232.865382	6115.056485	8.059878	-0.047335	4.228441
232.773409	6123.077017	8.064883	-0.047323	4.231112
233.209677	6131.119161	8.069888	-0.047410	4.233793
233.433708	6139.154868	8.074893	-0.047457	4.236469
233.502066	6147.094067	8.079898	-0.047475	4.239109
233.448563	6155.171420	8.084902	-0.047470	4.241792
233.592853	6163.108158	8.089907	-0.047502	4.244429
233.813743	6171.195499	8.094912	-0.047549	4.247115
233.730028	6179.207077	8.099917	-0.047538	4.249771
233.917926	6187.251939	8.104922	-0.047579	4.252439
234.130703	6195.306912	8.109926	-0.047624	4.255109
234.126577	6203.319173	8.114931	-0.047628	4.257761
234.504549	6211.302495	8.119936	-0.047704	4.260406
234.706005	6219.306071	8.124941	-0.047747	4.263054
234.733121	6227.299512	8.129946	-0.047757	4.265695
234.719420	6235.389805	8.134950	-0.047760	4.268366
234.976164	6243.368277	8.139955	-0.047813	4.271001
235.281678	6251.462262	8.144960	-0.047875	4.273673
235.383591	6259.477641	8.149965	-0.047899	4.276315
235.576866	6267.400860	8.154970	-0.047941	4.278926
235.849005	6275.449385	8.159974	-0.047997	4.281578
235.970683	6283.431825	8.164979	-0.048025	4.284205
236.261212	6291.480528	8.169984	-0.048084	4.286853
236.439096	6299.489612	8.174989	-0.048122	4.289486
236.606977	6307.512504	8.179994	-0.048159	4.292122
236.719553	6315.610285	8.184998	-0.048185	4.294780
236.719640	6323.578738	8.190003	-0.048191	4.297393
237.041947	6331.568094	8.195008	-0.048256	4.300014
236.965487	6339.610149	8.200013	-0.048247	4.302647
237.086327	6347.599948	8.205018	-0.048275	4.305263
237.436879	6355.617893	8.210022	-0.048345	4.307889
237.553026	6363.631070	8.215027	-0.048372	4.310510
237.526323	6371.701234	8.220032	-0.048373	4.313146
237.774476	6379.724113	8.225037	-0.048424	4.315768
237.830091	6387.658747	8.230042	-0.048440	4.318357
237.920635	6395.711338	8.235046	-0.048462	4.320984
237.965543	6403.703782	8.240051	-0.048476	4.323589
238.345838	6411.719515	8.245056	-0.048552	4.326203
238.367751	6419.717441	8.250061	-0.048561	4.328807
238.394797	6427.760404	8.255066	-0.048571	4.331424
238.626002	6435.812482	8.260070	-0.048620	4.334043
238.947325	6443.828199	8.265075	-0.048685	4.336650
238.802702	6451.824143	8.270080	-0.048663	4.339246
239.013400	6459.844296	8.275085	-0.048708	4.341850
239.146638	6467.794908	8.280090	-0.048738	4.344430
239.244552	6475.897472	8.285094	-0.048761	4.347057
239.247736	6483.834368	8.290099	-0.048767	4.349629
239.643169	6491.971551	8.295104	-0.048846	4.352266
239.908402	6500.046956	8.300109	-0.048901	4.354880
239.991533	6507.987049	8.305114	-0.048922	4.357449
240.148423	6515.991295	8.310118	-0.048956	4.360036
240.346257	6523.936722	8.315123	-0.048998	4.362604
240.487020	6531.952835	8.320128	-0.049030	4.365192
240.580244	6539.988231	8.325133	-0.049053	4.367785
240.940580	6547.950756	8.330138	-0.049125	4.370355
241.091978	6556.094540	8.335142	-0.049158	4.372980
241.047033	6564.047142	8.340147	-0.049155	4.375540
241.166855	6572.073184	8.345152	-0.049183	4.378124
241.094086	6580.063817	8.350157	-0.049175	4.380694
241.266164	6588.092624	8.355162	-0.049212	4.383276
241.599168	6596.124363	8.360166	-0.049279	4.385858
241.794881	6604.106967	8.365171	-0.049321	4.388422
241.955349	6612.144572	8.370176	-0.049356	4.391002
242.113668	6620.204541	8.375181	-0.049391	4.393588
242.363568	6628.207366	8.380186	-0.049443	4.396154
242.523219	6636.186262	8.385190	-0.049478	4.398710
242.513483	6644.206818	8.390195	-0.049481	4.401278
242.677344	6652.202867	8.395200	-0.049517	4.403837
242.924015	6660.237463	8.400205	-0.049569	4.406407
243.007521	6668.264803	8.405210	-0.049589	4.408973
243.079494	6676.316597	8.410214	-0.049608	4.411545
243.108915	6684.324870	8.415219	-0.049619	4.414101
243.248954	6692.383093	8.420224	-0.049650	4.416673
243.402794	6700.360648	8.425229	-0.049684	4.419217
243.522369	6708.374745	8.430234	-0.049712	4.421771
243.754614	6716.346753	8.435238	-0.049760	4.424311
243.756672	6724.343483	8.440243	-0.049766	4.426856
244.112578	6732.411399	8.445248	-0.049838	4.429423
244.289387	6740.480797	8.450253	-0.049876	4.431989
244.441728	6748.497298	8.455258	-0.049909	4.434537
244.476486	6756.537806	8.460262	-0.049921	4.437090
244.634750	6764.516334	8.465267	-0.049956	4.439623
244.809311	6772.509115	8.470272	-0.049994	4.442158
244.820513	6780.505747	8.475277	-0.050001	4.444693
244.999949	6788.520534	8.480282	-0.050040	4.447233
245.202310	6796.557442	8.485286	-0.050083	4.449778
245.273312	6804.572081	8.490291	-0.050101	4.452315
245.393308	6812.608490	8.495296	-0.050129	4.454857
245.533142	6820.635469	8.500301	-0.050160	4.457394
245.677729	6828.606722	8.505306	-0.050193	4.459913
245.889105	6836.657920	8.510310	-0.050237	4.462455
245.888256	6844.609385	8.515315	-0.050242	4.464964
245.904065	6852.681997	8.520320	-0.050251	4.467510
246.002525	6860.651279	8.525325	-0.050274	4.470022
246.125921	6868.719000	8.530330	-0.050303	4.472563
246.331315	6876.787498	8.535334	-0.050346	4.475104
246.424542	6884.754673	8.540339	-0.050369	4.477611
246.675964	6892.726680	8.545344	-0.050421	4.480119
246.938186	6900.771714	8.550349	-0.050475	4.482648
246.827940	6908.758558	8.555354	-0.050460	4.485156
247.080704	6916.818856	8.560359	-0.050512	4.487687
247.116721	6924.776428	8.565363	-0.050524	4.490184
247.373286	6932.850881	8.570368	-0.050577	4.492716
247.426806	6940.890043	8.575373	-0.050593	4.495236
247.600792	6948.867832	8.580378	-0.050630	4.497735
247.872175	6956.885178	8.585383	-0.050686	4.500245
247.785208	6964.905263	8.590387	-0.050675	4.502754
247.966061	6972.904529	8.595392	-0.050714	4.505256
248.223730	6980.925665	8.600397	-0.050767	4.507763
248.207225	6988.926621	8.605402	-0.050770	4.510262
248.360513	6997.031705	8.610407	-0.050804	4.512792
248.444321	7005.032838	8.615411	-0.050824	4.515289
248.631362	7013.000598	8.620416	-0.050865	4.517773
248.716694	7020.985604	8.625421	-0.050886	4.520262
248.888056	7028.964404	8.630426	-0.050923	4.522747
249.222411	7037.006720	8.635431	-0.050991	4.525251
248.983544	7045.042480	8.640435	-0.050951	4.527751
248.928429	7053.049238	8.645440	-0.050946	4.530240
249.158401	7061.101766	8.650445	-0.050995	4.532743
249.185148	7069.050515	8.655450	-0.051005	4.535212
249.594378	7077.107940	8.660455	-0.051086	4.537714
249.548636	7085.063931	8.665459	-0.051083	4.540182
249.782344	7093.119345	8.670464	-0.051132	4.542681
249.796277	7101.113985	8.675469	-0.051140	4.545158
249.828788	7109.160290	8.680474	-0.051151	4.547651
250.017361	7117.214275	8.685479	-0.051192	4.550144
250.175848	7125.211336	8.690483	-0.051226	4.552619
250.395609	7133.262016	8.695488	-0.051273	4.555108
250.595029	7141.248576	8.700493	-0.051315	4.557577
250.711004	7149.213623	8.705498	-0.051342	4.560037
250.871629	7157.243536	8.710503	-0.051377	4.562517
250.937867	7165.257000	8.715507	-0.051395	4.564989
251.166913	7173.304621	8.720512	-0.051443	4.567471
251.050539	7181.275857	8.725517	-0.051426	4.569928
251.215445	7189.347734	8.730522	-0.051462	4.572415
251.635413	7197.406040	8.735527	-0.051546	4.574896
251.644043	7205.388905	8.740531	-0.051553	4.577352
251.779163	7213.370648	8.745536	-0.051583	4.579807
251.685378	7221.422335	8.750541	-0.051571	4.582282
251.672951	7229.373455	8.755546	-0.051574	4.584725
251.986431	7237.474576	8.760551	-0.051638	4.587212
252.104161	7245.409647	8.765555	-0.051665	4.589647
252.321426	7253.514772	8.770560	-0.051711	4.592134
252.229663	7261.557629	8.775565	-0.051699	4.594599
252.515994	7269.563491	8.780570	-0.051758	4.597052
252.655976	7277.488255	8.785575	-0.051789	4.599479
252.695035	7285.572460	8.790579	-0.051802	4.601953
252.724865	7293.516076	8.795584	-0.051812	4.604383
252.958633	7301.584320	8.800589	-0.051861	4.606849
253.073891	7309.544612	8.805594	-0.051888	4.609282
253.376741	7317.628764	8.810599	-0.051950	4.611751
253.473989	7325.599717	8.815603	-0.051973	4.614184
253.631251	7333.677300	8.820608	-0.052008	4.616648
253.572620	7341.633208	8.825613	-0.052002	4.619074
253.586961	7349.660958	8.830618	-0.052010	4.621520
253.965941	7357.663524	8.835623	-0.052086	4.623957
253.918432	7365.697753	8.840627	-0.052082	4.626403
253.923613	7373.677780	8.845632	-0.052089	4.628831
254.132890	7381.789622	8.850637	-0.052133	4.631298
254.532772	7389.785960	8.855642	-0.052213	4.633728
254.714760	7397.820204	8.860647	-0.052252	4.636168
254.841951	7405.716710	8.865651	-0.052281	4.638566
255.056302	7413.786318	8.870656	-0.052326	4.641014
255.102932	7421.757952	8.875661	-0.052340	4.643432
255.122101	7429.791388	8.880666	-0.052349	4.645867
255.358882	7437.836861	8.885671	-0.052398	4.648305
255.340487	7445.824036	8.890675	-0.052400	4.650723
255.559727	7453.903814	8.895680	-0.052446	4.653168
255.742003	7461.915547	8.900685	-0.052486	4.655592
255.762339	7469.870025	8.905690	-0.052495	4.657997
255.760147	7477.913288	8.910695	-0.052499	4.660427
255.828668	7485.903129	8.915699	-0.052518	4.662840
255.983618	7493.907841	8.920704	-0.052552	4.665256
256.174833	7501.970750	8.925709	-0.052593	4.667688
256.423903	7509.940857	8.930714	-0.052644	4.670091
256.520731	7518.084393	8.935719	-0.052668	4.672546
256.766570	7526.109613	8.940723	-0.052719	4.674963
256.953342	7534.056849	8.945728	-0.052759	4.677355
257.057924	7542.073181	8.950733	-0.052784	4.679767
257.181802	7550.010738	8.955738	-0.052812	4.682154
257.244449	7558.024775	8.960743	-0.052829	4.684563
257.262280	7566.051022	8.965747	-0.052837	4.686975
257.749784	7574.065532	8.970752	-0.052934	4.689380
257.707341	7582.134118	8.975757	-0.052931	4.691802
257.599286	7590.138779	8.980762	-0.052916	4.694204
257.962926	7598.227699	8.985767	-0.052989	4.696628
257.864378	7606.120847	8.990771	-0.052976	4.698994
257.879912	7614.152194	8.995776	-0.052984	4.701399
258.072068	7622.148258	9.000781	-0.053025	4.703793
258.186797	7630.169820	9.005786	-0.053052	4.706192
258.504437	7638.182450	9.010791	-0.053117	4.708588
258.357780	7646.197768	9.015795	-0.053094	4.710984
258.483547	7654.231834	9.020800	-0.053123	4.713384
258.570046	7662.287509	9.025805	-0.053145	4.715789
258.718758	7670.263104	9.030810	-0.053178	4.718169
258.952860	7678.295866	9.035815	-0.053227	4.720565
258.964021	7686.281626	9.040819	-0.053234	4.722945
259.000171	7694.320906	9.045824	-0.053246	4.725341
259.077457	7702.366760	9.050829	-0.053266	4.727737
259.227866	7710.351328	9.055834	-0.053299	4.730114
259.580581	7718.410127	9.060839	-0.053370	4.732510
259.465292	7726.370944	9.065843	-0.053354	4.734878
259.811312	7734.433791	9.070848	-0.053424	4.737274
259.864627	7742.396989	9.075853	-0.053439	4.739639
259.886134	7750.398570	9.080858	-0.053448	4.742015
259.973447	7758.445909	9.085863	-0.053470	4.744403
260.085424	7766.475500	9.090867	-0.053496	4.746784
260.355294	7774.483509	9.095872	-0.053551	4.749158
260.434714	7782.495631	9.100877	-0.053571	4.751532
260.381002	7790.528221	9.105882	-0.053567	4.753911
260.640835	7798.589519	9.110887	-0.053620	4.756297
260.863661	7806.513114	9.115891	-0.053667	4.758640
260.909003	7814.561091	9.120896	-0.053681	4.761020
261.235748	7822.524602	9.125901	-0.053747	4.763373
261.452641	7830.556370	9.130906	-0.053793	4.765745
261.495497	7838.626021	9.135911	-0.053806	4.768128
261.507994	7846.574497	9.140915	-0.053814	4.770474
261.784103	7854.656256	9.145920	-0.053870	4.772857
261.696148	7862.636804	9.150925	-0.053859	4.775210
261.915808	7870.611559	9.155930	-0.053905	4.777559
262.125760	7878.695158	9.160935	-0.053950	4.779939
262.065419	7886.645544	9.165939	-0.053944	4.782280
262.218532	7894.688718	9.170944	-0.053978	4.784647
262.424971	7902.735627	9.175949	-0.054022	4.787012
262.625542	7910.752526	9.180954	-0.054064	4.789368
262.731036	7918.740205	9.185959	-0.054089	4.791715
262.870375	7926.744037	9.190963	-0.054120	4.794065
263.068977	7934.777203	9.195968	-0.054163	4.796422
263.167102	7942.796934	9.200973	-0.054186	4.798774
263.216581	7950.815647	9.205978	-0.054201	4.801125
263.357237	7958.817345	9.210983	-0.054232	4.803470
263.384732	7966.829781	9.215987	-0.054243	4.805817
263.697309	7974.851712	9.220992	-0.054306	4.808165
263.860943	7982.882783	9.225997	-0.054342	4.810514
263.902677	7990.262554	9.231002	-0.054355	4.812673
263.943435	7994.799697	9.236007	-0.054365	4.813999

263.819058	7997.377695	9.241011	-0.054344	4.814754
264.265413	7998.630295	9.246016	-0.054428	4.815118
264.244758	7999.074284	9.251021	-0.054424	4.815247
264.128565	8000.092447	9.256026	-0.054403	4.815546
264.479660	8000.155884	9.261031	-0.054469	4.815562
264.483456	8000.126045	9.266035	-0.054470	4.815554
264.311452	8000.151007	9.271040	-0.054438	4.815562
264.613869	8000.139944	9.276045	-0.054494	4.815557
264.677012	8000.092918	9.281050	-0.054506	4.815543
264.599725	8000.145067	9.286055	-0.054492	4.815559
264.631267	8000.122091	9.291059	-0.054498	4.815552
264.892854	8000.129588	9.296064	-0.054546	4.815553
264.809594	8000.144253	9.301069	-0.054531	4.815557
264.656913	8000.120396	9.306074	-0.054503	4.815551
264.787037	8000.157784	9.311079	-0.054527	4.815562
264.826719	8000.092214	9.316083	-0.054534	4.815542
264.860686	8000.087436	9.321088	-0.054541	4.815541
264.897658	8000.137185	9.326093	-0.054548	4.815555
264.833933	8000.094489	9.331098	-0.054536	4.815543
264.862567	8000.153715	9.336103	-0.054541	4.815560
264.949560	8000.118829	9.341107	-0.054558	4.815549
265.055756	8000.136598	9.346112	-0.054578	4.815554
265.123532	8000.150534	9.351117	-0.054590	4.815558
265.051506	8000.091679	9.356122	-0.054577	4.815541
265.151302	8000.111480	9.361127	-0.054596	4.815546
265.396925	8000.129397	9.366131	-0.054641	4.815550
265.407337	8000.125302	9.371136	-0.054643	4.815549
265.396803	8000.117659	9.376141	-0.054641	4.815547
265.248178	8000.117367	9.381146	-0.054614	4.815547
265.321748	8000.122852	9.386151	-0.054628	4.815549
265.447362	8000.116372	9.391155	-0.054651	4.815546
265.523046	8000.064209	9.396160	-0.054665	4.815531
265.413956	8000.100883	9.401165	-0.054645	4.815542
265.263677	8000.071724	9.406170	-0.054617	4.815534
265.419942	8000.125564	9.411175	-0.054646	4.815549
265.660123	8000.088915	9.416179	-0.054691	4.815537
265.534057	8000.080447	9.421184	-0.054668	4.815535
265.567216	8000.089543	9.426189	-0.054674	4.815538
265.497185	8000.029652	9.431194	-0.054661	4.815521
265.606371	8000.098744	9.436199	-0.054681	4.815540
265.537770	8000.086945	9.441203	-0.054669	4.815537
265.736227	8000.114772	9.446208	-0.054706	4.815544
265.857100	8000.115691	9.451213	-0.054728	4.815544
265.667743	8000.091231	9.456218	-0.054693	4.815538
265.591335	8000.116691	9.461223	-0.054679	4.815546
265.831636	8000.083249	9.466227	-0.054724	4.815535
265.766740	8000.075783	9.471232	-0.054712	4.815533
265.697525	8000.126997	9.476237	-0.054699	4.815548
265.624268	8000.083076	9.481242	-0.054685	4.815536
265.796667	8000.108340	9.486247	-0.054718	4.815542
265.710361	8000.095183	9.491251	-0.054702	4.815539
265.724205	8000.143485	9.496256	-0.054704	4.815553
265.700075	8000.135619	9.501261	-0.054700	4.815551
265.578111	8000.070604	9.506266	-0.054677	4.815532
265.685104	8000.145002	9.511271	-0.054697	4.815553
265.861888	8000.107314	9.516275	-0.054730	4.815542
265.928204	8000.066748	9.521280	-0.054743	4.815529
265.899789	8000.107949	9.526285	-0.054737	4.815542
265.963759	8000.086572	9.531290	-0.054749	4.815535
266.151042	8000.133445	9.536295	-0.054784	4.815548
266.057587	8000.119101	9.541299	-0.054767	4.815544
266.107456	8000.137017	9.546304	-0.054776	4.815549
266.177702	8000.163812	9.551309	-0.054790	4.815557
266.030622	8000.126158	9.556314	-0.054762	4.815546
266.217976	8000.122826	9.561319	-0.054797	4.815544
265.945675	8000.127984	9.566323	-0.054747	4.815547
266.030161	8000.143262	9.571328	-0.054762	4.815551
265.887809	8000.147345	9.576333	-0.054736	4.815553
265.773943	8000.126258	9.581338	-0.054715	4.815547
265.880015	8000.186755	9.586343	-0.054735	4.815565
265.800296	8000.140591	9.591347	-0.054720	4.815552
266.064054	8000.156671	9.596352	-0.054769	4.815555
266.221299	8000.169937	9.601357	-0.054799	4.815558
266.161994	8000.136926	9.606362	-0.054788	4.815549
266.245009	8000.168203	9.611367	-0.054803	4.815557
266.135014	8000.141838	9.616371	-0.054783	4.815550
266.053479	8000.120213	9.621376	-0.054768	4.815544
266.203779	8000.164343	9.626381	-0.054796	4.815557
266.009167	8000.114159	9.631386	-0.054759	4.815543
266.003940	8000.147195	9.636391	-0.054759	4.815552
265.956169	8000.127191	9.641395	-0.054750	4.815547
266.064015	8000.077692	9.646400	-0.054770	4.815532
266.148938	8000.117546	9.651405	-0.054786	4.815543
266.068122	8000.130115	9.656410	-0.054771	4.815547
266.110390	8000.163929	9.661415	-0.054779	4.815557
266.052402	8000.098893	9.666419	-0.054768	4.815538
266.051760	8000.109572	9.671424	-0.054768	4.815541
266.142450	8000.148452	9.676429	-0.054785	4.815552
266.238949	8000.107313	9.681434	-0.054803	4.815540
266.324973	8000.124753	9.686439	-0.054819	4.815544
266.292344	8000.104997	9.691443	-0.054813	4.815539
266.284448	8000.107011	9.696448	-0.054812	4.815539
266.508066	8000.124570	9.701453	-0.054853	4.815543
266.409656	8000.126168	9.706458	-0.054835	4.815544
266.522588	8000.142981	9.711463	-0.054856	4.815549
266.512960	8000.146035	9.716467	-0.054855	4.815550
266.316065	8000.119314	9.721472	-0.054818	4.815543
266.289346	8000.132770	9.726477	-0.054813	4.815547
266.262989	8000.109912	9.731482	-0.054808	4.815540
266.478085	8000.129468	9.736487	-0.054848	4.815545
266.338367	8000.106889	9.741491	-0.054823	4.815539
266.258538	8000.054313	9.746496	-0.054808	4.815524
266.411600	8000.155104	9.751501	-0.054836	4.815553
266.357467	8000.089063	9.756506	-0.054826	4.815534
266.352319	8000.144532	9.761511	-0.054825	4.815550
266.349004	8000.110302	9.766515	-0.054825	4.815540
266.408048	8000.073889	9.771520	-0.054836	4.815529
266.460806	8000.119626	9.776525	-0.054846	4.815542
266.509967	8000.107620	9.781530	-0.054855	4.815538
266.672965	8000.131664	9.786535	-0.054886	4.815545
266.515924	8000.125891	9.791539	-0.054856	4.815544
266.468138	8000.095205	9.796544	-0.054848	4.815535
266.650585	8000.131317	9.801549	-0.054882	4.815545
266.654104	8000.120700	9.806554	-0.054882	4.815542
266.631998	8000.163073	9.811559	-0.054878	4.815554
266.492662	8000.181092	9.816563	-0.054852	4.815560
266.632180	8000.139589	9.821568	-0.054878	4.815547
266.435577	8000.179102	9.826573	-0.054842	4.815560
266.400115	8000.145413	9.831578	-0.054835	4.815550
266.693745	8000.137414	9.836583	-0.054890	4.815546
266.518471	8000.108911	9.841587	-0.054858	4.815539
266.521810	8000.082267	9.846592	-0.054858	4.815531
266.542727	8000.123209	9.851597	-0.054862	4.815543
266.671209	8000.128527	9.856602	-0.054886	4.815544
266.596949	8000.131589	9.861607	-0.054873	4.815545
266.659894	8000.103786	9.866611	-0.054884	4.815537
266.799426	8000.095398	9.871616	-0.054910	4.815533
266.689479	8000.144877	9.876621	-0.054890	4.815548
266.714030	8000.083330	9.881626	-0.054895	4.815530
266.663603	8000.126307	9.886631	-0.054885	4.815543
266.545778	8000.158566	9.891635	-0.054864	4.815553
266.484235	8000.113767	9.896640	-0.054852	4.815540
266.494816	8000.136380	9.901645	-0.054854	4.815547
266.594024	8000.084602	9.906650	-0.054873	4.815531
266.482434	8000.102008	9.911655	-0.054852	4.815537
266.553271	8000.124540	9.916659	-0.054865	4.815543
266.602402	8000.150990	9.921664	-0.054875	4.815551
266.608552	8000.174598	9.926669	-0.054876	4.815557
266.434108	8000.125812	9.931674	-0.054843	4.815544
266.584652	8000.160333	9.936679	-0.054871	4.815553
266.532453	8000.147734	9.941683	-0.054862	4.815550
266.597898	8000.109290	9.946688	-0.054874	4.815538
266.695635	8000.140809	9.951693	-0.054892	4.815547
266.676531	8000.134094	9.956698	-0.054889	4.815545
266.756392	8000.161047	9.961703	-0.054904	4.815553
266.563202	8000.116226	9.966707	-0.054868	4.815541
266.649140	8000.083459	9.971712	-0.054884	4.815531
266.595842	8000.123185	9.976717	-0.054874	4.815542
266.586217	8000.095260	9.981722	-0.054872	4.815534
266.863796	8000.129728	9.986727	-0.054924	4.815543
266.807126	8000.152306	9.991731	-0.054914	4.815550
266.701146	8000.161258	9.996736	-0.054894	4.815553
266.670025	8000.182119	10.001741	-0.054888	4.815559
266.556099	8000.140734	10.006746	-0.054867	4.815548
266.623688	8000.178169	10.011751	-0.054880	4.815558
266.410118	8000.155446	10.016755	-0.054840	4.815553
266.722594	8000.144553	10.021760	-0.054898	4.815548
266.746203	8000.172721	10.026765	-0.054903	4.815556
266.738120	8000.153367	10.031770	-0.054902	4.815551
266.948983	8000.177127	10.036775	-0.054941	4.815557
266.930096	8000.138368	10.041779	-0.054937	4.815545
266.648021	8000.144433	10.046784	-0.054885	4.815548
266.753217	8000.148301	10.051789	-0.054905	4.815549
266.767177	8000.133582	10.056794	-0.054907	4.815545
266.744757	8000.168472	10.061799	-0.054903	4.815555
266.773238	8000.166810	10.066803	-0.054909	4.815554
266.727784	8000.173549	10.071808	-0.054900	4.815557
266.846049	8000.178700	10.076813	-0.054922	4.815557
266.689741	8000.172939	10.081818	-0.054893	4.815557
266.621570	8000.210284	10.086823	-0.054881	4.815568
266.628004	8000.175145	10.091827	-0.054882	4.815557
266.568841	8000.161364	10.096832	-0.054871	4.815554
266.890622	8000.179465	10.101837	-0.054931	4.815557
266.889144	8000.159151	10.106842	-0.054931	4.815552
266.986822	8000.185329	10.111847	-0.054949	4.815559
266.772421	8000.152979	10.116851	-0.054909	4.815550
266.860578	8000.174727	10.121856	-0.054926	4.815556
266.780140	8000.191575	10.126861	-0.054911	4.815562
266.725823	8000.140485	10.131866	-0.054901	4.815547
266.771384	8000.191445	10.136871	-0.054909	4.815562
266.807515	8000.159998	10.141875	-0.054916	4.815552
266.694484	8000.147469	10.146880	-0.054895	4.815549
266.716430	8000.148904	10.151885	-0.054899	4.815549
266.657555	8000.105217	10.156890	-0.054888	4.815537
266.602064	8000.180158	10.161895	-0.054878	4.815559
266.774047	8000.129574	10.166899	-0.054910	4.815543
266.734210	8000.118245	10.171904	-0.054903	4.815540
266.876756	8000.184683	10.176909	-0.054930	4.815559
266.771064	8000.156251	10.181914	-0.054910	4.815551
266.781327	8000.179927	10.186919	-0.054912	4.815558
266.993103	8000.167383	10.191923	-0.054952	4.815553
266.823464	8000.197724	10.196928	-0.054920	4.815563
266.787707	8000.225986	10.201933	-0.054913	4.815572
266.834720	8000.176557	10.206938	-0.054922	4.815557
266.950556	8000.172054	10.211943	-0.054944	4.815555
266.725922	8000.128854	10.216947	-0.054902	4.815543
266.788070	8000.156585	10.221952	-0.054914	4.815551
266.904381	8000.195887	10.226957	-0.054936	4.815562
266.684860	8000.144225	10.231962	-0.054895	4.815548
266.742692	8000.184704	10.236967	-0.054906	4.815560
266.958746	8000.177571	10.241971	-0.054946	4.815557
266.999723	8000.176113	10.246976	-0.054954	4.815556
267.052316	8000.194075	10.251981	-0.054964	4.815561
267.117221	8000.152416	10.256986	-0.054976	4.815548
267.124580	8000.189932	10.261991	-0.054977	4.815559
267.035343	8000.183135	10.266995	-0.054961	4.815558
267.013481	8000.141122	10.272000	-0.054957	4.815546
267.247951	8000.179157	10.277005	-0.055000	4.815556
267.046749	8000.140613	10.282010	-0.054963	4.815545
267.115558	8000.181273	10.287015	-0.054976	4.815557
267.230881	8000.173557	10.292019	-0.054997	4.815554
266.970164	8000.192790	10.297024	-0.054949	4.815561
266.941621	8000.203011	10.302029	-0.054944	4.815564
266.854952	8000.166345	10.307034	-0.054928	4.815554
266.999230	8000.186878	10.312039	-0.054955	4.815559
267.126941	8000.172955	10.317043	-0.054978	4.815554
267.048299	8000.178082	10.322048	-0.054964	4.815556
267.156833	8000.193756	10.327053	-0.054984	4.815560
266.914809	8000.149201	10.332058	-0.054939	4.815548
266.884448	8000.222418	10.337063	-0.054934	4.815570
267.065671	8000.166644	10.342067	-0.054967	4.815553
267.020064	8000.172312	10.347072	-0.054959	4.815555
266.931811	8000.161258	10.352077	-0.054943	4.815552
267.008849	8000.156119	10.357082	-0.054957	4.815550
267.100461	8000.186470	10.362087	-0.054974	4.815558
266.955728	8000.189445	10.367091	-0.054947	4.815560
267.033032	8000.160809	10.372096	-0.054962	4.815551
267.192886	8000.199757	10.377101	-0.054992	4.815562
267.065106	8000.119688	10.382106	-0.054968	4.815539
267.165056	8000.177950	10.387111	-0.054987	4.815556
267.079943	8000.175493	10.392115	-0.054971	4.815555
266.984221	8000.157907	10.397120	-0.054953	4.815551
267.116610	8000.192132	10.402125	-0.054978	4.815560
267.090986	8000.131897	10.407130	-0.054973	4.815542
267.104524	8000.163105	10.412135	-0.054976	4.815552
267.090681	8000.157544	10.417139	-0.054973	4.815550
267.057128	8000.139909	10.422144	-0.054967	4.815545
267.227685	8000.144849	10.427149	-0.054999	4.815546
267.091436	8000.104165	10.432154	-0.054974	4.815534
267.079623	8000.140298	10.437159	-0.054971	4.815545
267.156268	8000.135153	10.442163	-0.054986	4.815543
267.347959	8000.157531	10.447168	-0.055022	4.815549
267.248835	8000.206120	10.452173	-0.055003	4.815563
266.986377	8000.161230	10.457178	-0.054954	4.815552
267.288757	8000.183287	10.462183	-0.055011	4.815557
267.111248	8000.186793	10.467187	-0.054978	4.815558
266.985931	8000.159107	10.472192	-0.054955	4.815551
267.180694	8000.186877	10.477197	-0.054991	4.815558
267.214429	8000.143639	10.482202	-0.054997	4.815545
267.215486	8000.140459	10.487207	-0.054998	4.815544
267.082695	8000.129742	10.492211	-0.054973	4.815542
267.155119	8000.110641	10.497216	-0.054986	4.815536
267.365866	8000.189948	10.502221	-0.055026	4.815558
267.036584	8000.127939	10.507226	-0.054965	4.815542
267.206187	8000.165979	10.512231	-0.054996	4.815552
267.238657	8000.154767	10.517235	-0.055002	4.815548
267.046856	8000.162312	10.522240	-0.054967	4.815552
267.342069	8000.166091	10.527245	-0.055022	4.815551
267.192823	8000.141218	10.532250	-0.054994	4.815545
266.981838	8000.150584	10.537255	-0.054955	4.815548
267.161550	8000.167425	10.542259	-0.054988	4.815552
267.092623	8000.166301	10.547264	-0.054976	4.815552
267.271653	8000.198087	10.552269	-0.055009	4.815561
267.215821	8000.138425	10.557274	-0.054999	4.815544
267.295996	8000.180340	10.562279	-0.055014	4.815556
267.280204	8000.162996	10.567283	-0.055011	4.815551
267.246519	8000.093015	10.572288	-0.055005	4.815530
267.262310	8000.154170	10.577293	-0.055008	4.815548
267.351716	8000.140688	10.582298	-0.055024	4.815544
267.368600	8000.181565	10.587303	-0.055028	4.815556
267.111445	8000.178423	10.592307	-0.054980	4.815556
267.214916	8000.173717	10.597312	-0.054999	4.815554
267.312680	8000.182805	10.602317	-0.055017	4.815556
267.126642	8000.175488	10.607322	-0.054983	4.815555
267.093339	8000.093763	10.612327	-0.054977	4.815531
267.497138	8000.129234	10.617331	-0.055052	4.815540
267.274874	8000.135210	10.622336	-0.055011	4.815542
267.424321	8000.176125	10.627341	-0.055039	4.815554
267.311885	8000.150786	10.632346	-0.055018	4.815547
267.226555	8000.172895	10.637351	-0.055002	4.815554
267.139818	8000.162934	10.642355	-0.054986	4.815551
267.255871	8000.163776	10.647360	-0.055008	4.815551
267.357471	8000.177199	10.652365	-0.055027	4.815554
267.186014	8000.158371	10.657370	-0.054995	4.815550
267.100497	8000.196500	10.662375	-0.054979	4.815561
267.176076	8000.189201	10.667379	-0.054993	4.815559
267.187301	8000.162686	10.672384	-0.054995	4.815551
267.341709	8000.200477	10.677389	-0.055024	4.815561
267.253120	8000.136005	10.682394	-0.055008	4.815543
267.439070	8000.166835	10.687399	-0.055042	4.815551
267.427466	8000.173061	10.692403	-0.055040	4.815553
267.454584	8000.186332	10.697408	-0.055045	4.815557
267.368140	8000.205218	10.702413	-0.055029	4.815562
267.138499	8000.155524	10.707418	-0.054987	4.815549
267.187080	8000.167010	10.712423	-0.054996	4.815552
267.198080	8000.204586	10.717427	-0.054998	4.815563
267.181581	8000.179753	10.722432	-0.054995	4.815556
267.227138	8000.186916	10.727437	-0.055004	4.815558
267.122194	8000.154223	10.732442	-0.054984	4.815549
267.400035	8000.158787	10.737447	-0.055036	4.815549
267.389599	8000.175714	10.742451	-0.055034	4.815554
267.214526	8000.164304	10.747456	-0.055001	4.815551
267.581541	8000.200241	10.752461	-0.055070	4.815560
267.298605	8000.190266	10.757466	-0.055017	4.815558
267.425399	8000.206240	10.762471	-0.055041	4.815562
267.322996	8000.173588	10.767475	-0.055022	4.815553
267.331642	8000.180146	10.772480	-0.055024	4.815555
267.376316	8000.200114	10.777485	-0.055032	4.815561
267.293917	8000.126130	10.782490	-0.055017	4.815540
267.575912	8000.119010	10.787495	-0.055069	4.815536
267.461601	8000.165214	10.792499	-0.055048	4.815550
267.127709	8000.170427	10.797504	-0.054986	4.815553
267.465952	8000.163162	10.802509	-0.055049	4.815550
267.204059	8000.173830	10.807514	-0.055000	4.815554
267.224614	8000.198743	10.812519	-0.055004	4.815561
267.268595	8000.191994	10.817523	-0.055013	4.815559
267.197431	8000.201516	10.822528	-0.055000	4.815562
267.450441	8000.174693	10.827533	-0.055047	4.815553
267.364336	8000.133763	10.832538	-0.055031	4.815542
267.504337	8000.223662	10.837543	-0.055057	4.815567
267.409113	8000.213561	10.842547	-0.055039	4.815565
267.166984	8000.183959	10.847552	-0.054994	4.815557
267.430574	8000.203245	10.852557	-0.055043	4.815562
267.388319	8000.156624	10.857562	-0.055036	4.815548
267.399150	8000.182446	10.862567	-0.055038	4.815556
267.501708	8000.184135	10.867571	-0.055057	4.815556
267.562681	8000.188347	10.872576	-0.055068	4.815557
267.327685	8000.216547	10.877581	-0.055025	4.815566
267.304805	8000.173449	10.882586	-0.055020	4.815553
267.470568	8000.163356	10.887591	-0.055051	4.815550
267.526922	8000.184584	10.892595	-0.055062	4.815556
267.390920	8000.178087	10.897600	-0.055037	4.815554
267.508351	8000.212067	10.902605	-0.055059	4.815564
267.349015	8000.180618	10.907610	-0.055029	4.815555
267.355153	8000.192476	10.912615	-0.055030	4.815559
267.351771	8000.155039	10.917619	-0.055030	4.815548
267.443019	8000.154406	10.922624	-0.055047	4.815547
267.407849	8000.179474	10.927629	-0.055040	4.815555
267.295069	8000.177632	10.932634	-0.055019	4.815555
267.436803	8000.191714	10.937639	-0.055046	4.815558
267.568263	8000.214174	10.942643	-0.055070	4.815564
267.466459	8000.182600	10.947648	-0.055052	4.815555
267.601179	8000.209386	10.952653	-0.055077	4.815562
267.432626	8000.169240	10.957658	-0.055045	4.815552
267.345639	8000.223369	10.962663	-0.055029	4.815568
267.477720	8000.195631	10.967667	-0.055054	4.815559
267.382234	8000.170571	10.972672	-0.055036	4.815552
267.556878	8000.183056	10.977677	-0.055069	4.815555
267.405532	8000.159216	10.982682	-0.055041	4.815549
267.481351	8000.165807	10.987687	-0.055055	4.815550
267.487437	8000.140276	10.992691	-0.055056	4.815543
267.385618	8000.135409	10.997696	-0.055037	4.815542
267.362469	8000.199130	11.002701	-0.055033	4.815561
267.452407	8000.183521	11.007706	-0.055050	4.815556
267.368923	8000.187499	11.012711	-0.055034	4.815557
267.316358	8000.189849	11.017715	-0.055025	4.815558
267.431831	8000.176794	11.022720	-0.055046	4.815554
267.482298	8000.173356	11.027725	-0.055056	4.815552
267.398083	8000.146344	11.032730	-0.055040	4.815545
267.442043	8000.168437	11.037735	-0.055048	4.815551
267.627832	8000.170422	11.042739	-0.055083	4.815551
267.340670	8000.147560	11.047744	-0.055030	4.815546
267.388720	8000.168651	11.052749	-0.055039	4.815552
267.366057	8000.123420	11.057754	-0.055035	4.815538
267.396233	8000.146355	11.062759	-0.055040	4.815545
267.427053	8000.179983	11.067763	-0.055046	4.815555
267.588741	8000.166618	11.072768	-0.055076	4.815550
267.511315	8000.205949	11.077773	-0.055062	4.815562
267.289904	8000.177754	11.082778	-0.055021	4.815555
267.614327	8000.204447	11.087783	-0.055081	4.815561
267.533791	8000.196724	11.092787	-0.055066	4.815559
267.485998	8000.145739	11.097792	-0.055058	4.815544
267.612571	8000.179869	11.102797	-0.055081	4.815554
267.589713	8000.130362	11.107802	-0.055077	4.815539
267.473325	8000.118846	11.112807	-0.055055	4.815537
267.695546	8000.153477	11.117811	-0.055097	4.815546
267.619711	8000.150103	11.122816	-0.055083	4.815545
267.602329	8000.167985	11.127821	-0.055080	4.815550
267.534854	8000.156203	11.132826	-0.055067	4.815547
267.610725	8000.162796	11.137831	-0.055081	4.815549
267.538775	8000.194738	11.142835	-0.055068	4.815558
267.533581	8000.173295	11.147840	-0.055067	4.815552
267.555887	8000.161917	11.152845	-0.055071	4.815549
267.516724	8000.152736	11.157850	-0.055064	4.815546
267.500688	8000.167435	11.162855	-0.055061	4.815551
267.480791	8000.170320	11.167859	-0.055058	4.815552
267.594217	8000.120912	11.172864	-0.055079	4.815537
267.639186	8000.161181	11.177869	-0.055087	4.815548
267.534213	8000.174422	11.182874	-0.055068	4.815552
267.655737	8000.146511	11.187879	-0.055091	4.815544
267.673204	8000.170306	11.192883	-0.055094	4.815551
267.737952	8000.143600	11.197888	-0.055106	4.815542
267.821113	8000.185565	11.202893	-0.055122	4.815554
267.456256	8000.152881	11.207898	-0.055054	4.815547
267.459547	8000.170034	11.212903	-0.055054	4.815552
267.743439	8000.144786	11.217907	-0.055107	4.815543
267.804576	8000.131909	11.222912	-0.055119	4.815539
267.675393	8000.175732	11.227917	-0.055095	4.815552
267.547763	8000.172577	11.232922	-0.055071	4.815552
267.610524	8000.197115	11.237927	-0.055083	4.815559
267.814703	8000.199403	11.242931	-0.055121	4.815558
267.599040	8000.160620	11.247936	-0.055081	4.815548
267.599644	8000.189479	11.252941	-0.055081	4.815557
267.497350	8000.170716	11.257946	-0.055062	4.815552
267.609488	8000.129833	11.262951	-0.055083	4.815539
267.557174	8000.142869	11.267955	-0.055073	4.815543
267.505987	8000.103579	11.272960	-0.055064	4.815532
267.723586	8000.148817	11.277965	-0.055105	4.815544
267.479833	8000.111710	11.282970	-0.055059	4.815534
267.585194	8000.150834	11.287975	-0.055079	4.815545
267.758569	8000.166503	11.292979	-0.055111	4.815549
267.468994	8000.122236	11.297984	-0.055057	4.815537
267.657103	8000.157375	11.302989	-0.055093	4.815547
267.645769	8000.139036	11.307994	-0.055091	4.815542
267.599513	8000.142557	11.312999	-0.055082	4.815543
267.472228	8000.145818	11.318003	-0.055058	4.815544
267.480975	8000.116057	11.323008	-0.055060	4.815536
267.802014	8000.188630	11.328013	-0.055120	4.815555
267.676836	8000.158809	11.333018	-0.055097	4.815547
267.681151	8000.152477	11.338023	-0.055098	4.815545
267.730440	8000.186408	11.343027	-0.055107	4.815555
267.674683	8000.157726	11.348032	-0.055097	4.815547
268.021747	8000.205088	11.353037	-0.055161	4.815559
267.894903	8000.157079	11.358042	-0.055138	4.815546
267.636962	8000.176356	11.363047	-0.055090	4.815552
267.673587	8000.198329	11.368051	-0.055097	4.815559
267.693303	8000.185840	11.373056	-0.055100	4.815555
267.683678	8000.217737	11.378061	-0.055099	4.815564
267.510372	8000.173239	11.383066	-0.055067	4.815552
267.478825	8000.188753	11.388071	-0.055061	4.815557
267.727770	8000.192843	11.393075	-0.055107	4.815557
267.713913	8000.161643	11.398080	-0.055105	4.815548
267.717376	8000.189482	11.403085	-0.055105	4.815556
267.751358	8000.143043	11.408090	-0.055112	4.815542
267.815889	8000.125948	11.413095	-0.055124	4.815537
267.788061	8000.149000	11.418099	-0.055119	4.815544
267.617222	8000.148341	11.423104	-0.055087	4.815544
267.813063	8000.197495	11.428109	-0.055124	4.815558
267.763919	8000.188150	11.433114	-0.055115	4.815555
267.797451	8000.180161	11.438119	-0.055121	4.815553
268.003659	8000.186755	11.443123	-0.055159	4.815554
267.774052	8000.134924	11.448128	-0.055117	4.815540
267.826686	8000.148614	11.453133	-0.055127	4.815543
267.854291	8000.165097	11.458138	-0.055132	4.815548
267.788355	8000.185388	11.463143	-0.055120	4.815554
267.859222	8000.169465	11.468147	-0.055133	4.815549
267.637508	8000.153016	11.473152	-0.055092	4.815546
267.764144	8000.191421	11.478157	-0.055115	4.815556
267.728428	8000.170545	11.483162	-0.055109	4.815550
267.663532	8000.178033	11.488167	-0.055097	4.815553
267.938936	8000.212469	11.493171	-0.055148	4.815562
268.003352	8000.161188	11.498176	-0.055160	4.815546
267.886623	8000.202011	11.503181	-0.055139	4.815559
267.958216	8000.158325	11.508186	-0.055152	4.815546
267.903361	8000.201231	11.513191	-0.055142	4.815558
267.806464	8000.182556	11.518195	-0.055124	4.815553
267.573975	8000.160589	11.523200	-0.055081	4.815548
267.860413	8000.201615	11.528205	-0.055134	4.815559
267.889350	8000.189278	11.533210	-0.055139	4.815555
267.734980	8000.161114	11.538215	-0.055111	4.815547
267.795230	8000.169587	11.543219	-0.055122	4.815550
267.888964	8000.185019	11.548224	-0.055140	4.815554
267.683147	8000.192332	11.553229	-0.055101	4.815557
267.651405	8000.143747	11.558234	-0.055096	4.815543
267.793576	8000.174929	11.563239	-0.055122	4.815551
267.753223	8000.176411	11.568243	-0.055115	4.815552
267.905461	8000.145799	11.573248	-0.055143	4.815542
268.022914	8000.195804	11.578253	-0.055165	4.815556
267.923438	8000.187770	11.583258	-0.055147	4.815554
267.872879	8000.185879	11.588263	-0.055137	4.815554
268.043448	8000.202571	11.593267	-0.055169	4.815558
267.914699	8000.159872	11.598272	-0.055145	4.815546
267.799359	8000.193240	11.603277	-0.055124	4.815557
267.708079	8000.186408	11.608282	-0.055107	4.815555
267.912239	8000.134215	11.613287	-0.055145	4.815539
267.982077	8000.172756	11.618291	-0.055158	4.815550
267.738751	8000.140997	11.623296	-0.055113	4.815542
267.873074	8000.153890	11.628301	-0.055138	4.815545
267.902198	8000.170398	11.633306	-0.055143	4.815549
267.684590	8000.186064	11.638311	-0.055103	4.815555
267.764394	8000.184175	11.643315	-0.055118	4.815554
267.796834	8000.188988	11.648320	-0.055124	4.815555
267.717758	8000.198380	11.653325	-0.055109	4.815558
267.777428	8000.170523	11.658330	-0.055121	4.815550
267.930194	8000.146329	11.663335	-0.055149	4.815542
267.968798	8000.193973	11.668339	-0.055156	4.815556
267.756593	8000.132813	11.673344	-0.055117	4.815539
267.809994	8000.174289	11.678349	-0.055127	4.815551
268.022717	8000.160694	11.683354	-0.055167	4.815546
267.892247	8000.153219	11.688359	-0.055142	4.815544
268.038385	8000.218651	11.693363	-0.055170	4.815563
267.949182	8000.164849	11.698368	-0.055153	4.815547
267.908129	8000.216528	11.703373	-0.055146	4.815563
267.754141	8000.221486	11.708378	-0.055117	4.815565
267.742859	8000.195670	11.713383	-0.055115	4.815557
267.807892	8000.170037	11.718387	-0.055127	4.815550
267.571343	8000.170437	11.723392	-0.055083	4.815551
267.746372	8000.200021	11.728397	-0.055116	4.815559
267.689930	8000.172396	11.733402	-0.055105	4.815551
267.625162	8000.188433	11.738407	-0.055094	4.815556
267.816744	8000.181968	11.743411	-0.055129	4.815553
267.775065	8000.172745	11.748416	-0.055122	4.815551
267.862811	8000.162440	11.753421	-0.055138	4.815547
267.698483	8000.157615	11.758426	-0.055107	4.815547
267.885155	8000.161753	11.763431	-0.055142	4.815547
268.024231	8000.193952	11.768435	-0.055168	4.815556
267.945967	8000.151013	11.773440	-0.055154	4.815543
267.984915	8000.175161	11.778445	-0.055161	4.815550
267.964962	8000.164158	11.783450	-0.055157	4.815547
267.865172	8000.171074	11.788455	-0.055139	4.815550
267.813737	8000.179851	11.793459	-0.055129	4.815552
267.650172	8000.166493	11.798464	-0.055099	4.815549
267.888217	8000.186428	11.803469	-0.055144	4.815554
267.755639	8000.159690	11.808474	-0.055119	4.815547
267.682820	8000.170254	11.813479	-0.055105	4.815550
267.882501	8000.192765	11.818483	-0.055143	4.815556
267.624433	8000.151150	11.823488	-0.055095	4.815545
267.825521	8000.138431	11.828493	-0.055132	4.815540
267.826746	8000.169437	11.833498	-0.055133	4.815549
267.866334	8000.205346	11.838503	-0.055140	4.815560
267.993903	8000.217060	11.843507	-0.055164	4.815562
267.930271	8000.185044	11.848512	-0.055152	4.815553
268.005723	8000.206585	11.853517	-0.055166	4.815559
267.979969	8000.138869	11.858522	-0.055161	4.815540
267.816513	8000.139400	11.863527	-0.055131	4.815541
267.797760	8000.174352	11.868531	-0.055128	4.815551
267.611521	8000.187327	11.873536	-0.055093	4.815556
267.787093	8000.204102	11.878541	-0.055126	4.815560
267.989330	8000.177515	11.883546	-0.055164	4.815551
267.836783	8000.167542	11.888551	-0.055135	4.815549
268.067533	8000.160651	11.893555	-0.055178	4.815546
268.035136	8000.171878	11.898560	-0.055172	4.815549
268.221172	8000.215531	11.903565	-0.055207	4.815561
267.931170	8000.180869	11.908570	-0.055153	4.815552
267.917870	8000.155019	11.913575	-0.055151	4.815545
268.062227	8000.183032	11.918579	-0.055178	4.815552
268.036574	8000.146298	11.923584	-0.055173	4.815542
268.118766	8000.180769	11.928589	-0.055188	4.815551
268.005114	8000.166092	11.933594	-0.055167	4.815547
267.816453	8000.167277	11.938599	-0.055132	4.815549
267.894823	8000.185662	11.943603	-0.055147	4.815554
267.904958	8000.103579	11.948608	-0.055149	4.815530
268.044712	8000.181725	11.953613	-0.055175	4.815552
267.946112	8000.163022	11.958618	-0.055157	4.815547
267.859473	8000.155199	11.963623	-0.055141	4.815545
268.036081	8000.190150	11.968627	-0.055174	4.815554
268.028403	8000.145164	11.973632	-0.055172	4.815541
268.055922	8000.208650	11.978637	-0.055178	4.815560
267.982796	8000.157249	11.983642	-0.055164	4.815545
268.026763	8000.154773	11.988647	-0.055172	4.815544
267.962395	8000.191113	11.993651	-0.055160	4.815555
267.997200	8000.178872	11.998656	-0.055167	4.815551
268.052446	8000.179785	12.003661	-0.055177	4.815551
267.907223	8000.173136	12.008666	-0.055150	4.815550
268.019650	8000.169646	12.013671	-0.055171	4.815548
268.249674	8000.197997	12.018675	-0.055214	4.815556
268.034730	8000.170976	12.023680	-0.055174	4.815549
268.189502	8000.232277	12.028685	-0.055203	4.815566
267.966568	8000.175213	12.033690	-0.055162	4.815550
268.075050	8000.198365	12.038695	-0.055182	4.815557
268.105806	8000.190330	12.043699	-0.055188	4.815554
267.927100	8000.146811	12.048704	-0.055155	4.815542
268.075498	8000.202666	12.053709	-0.055182	4.815558
268.005479	8000.176954	12.058714	-0.055169	4.815551
267.835833	8000.186997	12.063719	-0.055138	4.815554
267.997614	8000.206750	12.068723	-0.055168	4.815559
267.886788	8000.163277	12.073728	-0.055147	4.815547
267.964327	8000.179511	12.078733	-0.055162	4.815552
267.879020	8000.165300	12.083738	-0.055146	4.815548
267.985612	8000.174533	12.088743	-0.055166	4.815550
268.254008	8000.190694	12.093747	-0.055216	4.815553
268.011029	8000.141848	12.098752	-0.055171	4.815540
268.006363	8000.156734	12.103757	-0.055170	4.815545
268.112345	8000.175572	12.108762	-0.055190	4.815550
267.959731	8000.184826	12.113767	-0.055162	4.815553
267.928188	8000.199271	12.118771	-0.055156	4.815557
268.006929	8000.186682	12.123776	-0.055171	4.815553
268.060607	8000.216413	12.128781	-0.055181	4.815562
268.088216	8000.194439	12.133786	-0.055186	4.815555
268.120704	8000.207798	12.138791	-0.055192	4.815559
268.169248	8000.192578	12.143795	-0.055201	4.815554
267.918819	8000.154292	12.148800	-0.055155	4.815544
267.912821	8000.168088	12.153805	-0.055154	4.815548
268.080309	8000.144136	12.158810	-0.055185	4.815541
267.976178	8000.171277	12.163815	-0.055166	4.815549
268.132054	8000.216572	12.168819	-0.055195	4.815562
268.140741	8000.166513	12.173824	-0.055196	4.815547
268.269959	8000.185732	12.178829	-0.055220	4.815552
268.076950	8000.179368	12.183834	-0.055185	4.815551
268.017596	8000.167718	12.188839	-0.055174	4.815548
268.135827	8000.182484	12.193843	-0.055196	4.815552
267.985694	8000.164004	12.198848	-0.055168	4.815547
268.101350	8000.180864	12.203853	-0.055189	4.815551
268.283079	8000.160351	12.208858	-0.055223	4.815544
268.201723	8000.177183	12.213863	-0.055208	4.815550
268.088285	8000.198831	12.218867	-0.055187	4.815557
268.036771	8000.170218	12.223872	-0.055178	4.815548
268.159894	8000.209634	12.228877	-0.055201	4.815559
268.078318	8000.199756	12.233882	-0.055186	4.815557
268.163271	8000.178724	12.238887	-0.055202	4.815550
268.357163	8000.208618	12.243891	-0.055238	4.815558
268.238481	8000.186381	12.248896	-0.055216	4.815552
268.195762	8000.219872	12.253901	-0.055208	4.815562
268.441991	8000.221782	12.258906	-0.055254	4.815562
268.131107	8000.210278	12.263911	-0.055196	4.815560
268.098833	8000.223643	12.268915	-0.055190	4.815564
268.096802	8000.137087	12.273920	-0.055190	4.815538
268.167617	8000.173509	12.278925	-0.055203	4.815549
268.145552	8000.174222	12.283930	-0.055199	4.815549
268.078774	8000.195567	12.288935	-0.055187	4.815556
268.110357	8000.190751	12.293939	-0.055193	4.815554
268.290338	8000.183028	12.298944	-0.055226	4.815551
268.062389	8000.173954	12.303949	-0.055184	4.815549
268.217827	8000.157282	12.308954	-0.055213	4.815544
268.181093	8000.172710	12.313959	-0.055206	4.815548
268.219161	8000.201117	12.318963	-0.055213	4.815557
268.323029	8000.165438	12.323968	-0.055233	4.815546
268.299228	8000.198171	12.328973	-0.055228	4.815555
268.150607	8000.174374	12.333978	-0.055201	4.815549
268.037614	8000.173596	12.338983	-0.055180	4.815549
268.347523	8000.192575	12.343987	-0.055238	4.815553
268.070549	8000.141034	12.348992	-0.055186	4.815540
268.053024	8000.162118	12.353997	-0.055183	4.815546
268.225131	8000.173495	12.359002	-0.055215	4.815548
268.329975	8000.173086	12.364007	-0.055235	4.815548
268.141984	8000.199920	12.369011	-0.055200	4.815557
268.156027	8000.191611	12.374016	-0.055202	4.815554
268.201790	8000.244714	12.379021	-0.055211	4.815569
268.034576	8000.203519	12.384026	-0.055180	4.815558
267.986989	8000.146128	12.389031	-0.055171	4.815542
268.090303	8000.193765	12.394035	-0.055190	4.815555
267.903453	8000.156522	12.399040	-0.055156	4.815545
267.992658	8000.170812	12.404045	-0.055172	4.815549
268.245877	8000.196338	12.409050	-0.055220	4.815555
268.158298	8000.179952	12.414055	-0.055203	4.815551
268.191899	8000.205081	12.419059	-0.055210	4.815558
268.049430	8000.182453	12.424064	-0.055183	4.815552
268.236742	8000.235742	12.429069	-0.055218	4.815567
268.235942	8000.209029	12.434074	-0.055218	4.815559
267.948980	8000.211806	12.439079	-0.055165	4.815561
268.080425	8000.238539	12.444083	-0.055189	4.815568
268.047074	8000.208088	12.449088	-0.055183	4.815559
267.969869	8000.161961	12.454093	-0.055169	4.815546
268.067823	8000.176394	12.459098	-0.055187	4.815550
268.035789	8000.166261	12.464103	-0.055181	4.815547
268.034462	8000.163041	12.469107	-0.055181	4.815546
268.189922	8000.169872	12.474112	-0.055210	4.815547
268.350869	8000.113765	12.479117	-0.055240	4.815530
268.187095	8000.152747	12.484122	-0.055210	4.815542
268.162980	8000.140607	12.489127	-0.055205	4.815539
268.307558	8000.187853	12.494131	-0.055232	4.815552
268.240884	8000.156855	12.499136	-0.055220	4.815543
268.263777	8000.194627	12.504141	-0.055224	4.815554
268.284638	8000.169338	12.509146	-0.055228	4.815547
268.260010	8000.153985	12.514151	-0.055224	4.815542
268.205092	8000.170183	12.519155	-0.055214	4.815547
268.107914	8000.149367	12.524160	-0.055196	4.815542
268.124651	8000.179560	12.529165	-0.055199	4.815551
268.154763	8000.183265	12.534170	-0.055205	4.815552
268.234137	8000.154663	12.539175	-0.055219	4.815543
268.258789	8000.191396	12.544179	-0.055224	4.815553
268.330880	8000.140240	12.549184	-0.055238	4.815538
268.359454	8000.171696	12.554189	-0.055243	4.815547
268.442390	8000.173063	12.559194	-0.055259	4.815547
268.272845	8000.176698	12.564199	-0.055227	4.815549
268.232208	8000.169629	12.569203	-0.055220	4.815547
268.275782	8000.182102	12.574208	-0.055228	4.815551
268.429700	8000.217750	12.579213	-0.055257	4.815560
268.372993	8000.213622	12.584218	-0.055246	4.815559
268.046465	8000.180497	12.589223	-0.055185	4.815551
268.198396	8000.170177	12.594227	-0.055214	4.815547
268.144888	8000.150077	12.599232	-0.055204	4.815542
268.249497	8000.179575	12.604237	-0.055223	4.815550
268.301132	8000.216751	12.609242	-0.055233	4.815561
268.266785	8000.171327	12.614247	-0.055227	4.815547
268.263766	8000.202264	12.619251	-0.055226	4.815557
268.137094	8000.164940	12.624256	-0.055203	4.815546
268.103964	8000.206065	12.629261	-0.055197	4.815558
268.064501	8000.147739	12.634266	-0.055189	4.815542
268.087866	8000.178040	12.639271	-0.055194	4.815550
268.328672	8000.202295	12.644275	-0.055239	4.815556
268.347852	8000.163091	12.649280	-0.055242	4.815545
268.434430	8000.194430	12.654285	-0.055259	4.815553
268.347323	8000.193007	12.659290	-0.055242	4.815553
268.478959	8000.172741	12.664295	-0.055267	4.815547
268.379801	8000.148687	12.669299	-0.055249	4.815540
268.403140	8000.171510	12.674304	-0.055253	4.815547
268.264627	8000.208771	12.679309	-0.055227	4.815558
268.121096	8000.167965	12.684314	-0.055201	4.815547
268.211487	8000.195093	12.689319	-0.055218	4.815555
268.492307	8000.194367	12.694323	-0.055270	4.815553
268.155376	8000.184572	12.699328	-0.055207	4.815552
268.066307	8000.197005	12.704333	-0.055191	4.815556
268.369391	8000.182756	12.709338	-0.055247	4.815550
268.323716	8000.170263	12.714343	-0.055239	4.815547
268.479026	8000.212344	12.719347	-0.055268	4.815558
268.471793	8000.197276	12.724352	-0.055267	4.815554
268.348849	8000.202744	12.729357	-0.055244	4.815556
268.506274	8000.187173	12.734362	-0.055273	4.815551
268.421513	8000.159083	12.739367	-0.055257	4.815543
268.439474	8000.206388	12.744371	-0.055261	4.815557
268.423723	8000.192249	12.749376	-0.055258	4.815553
268.380324	8000.203295	12.754381	-0.055250	4.815556
268.352668	8000.207121	12.759386	-0.055245	4.815557
268.267769	8000.166209	12.764391	-0.055229	4.815546
268.313184	8000.221443	12.769395	-0.055238	4.815562
268.228730	8000.158105	12.774400	-0.055222	4.815544
268.384108	8000.210870	12.779405	-0.055251	4.815558
268.380251	8000.196926	12.784410	-0.055251	4.815554
268.321039	8000.182073	12.789415	-0.055240	4.815550
268.437018	8000.166891	12.794419	-0.055261	4.815545
268.411630	8000.151526	12.799424	-0.055257	4.815541
268.538117	8000.187793	12.804429	-0.055280	4.815551
268.576788	8000.201254	12.809434	-0.055288	4.815555
268.466164	8000.212265	12.814439	-0.055267	4.815558
268.455690	8000.232397	12.819443	-0.055265	4.815564
268.410887	8000.180391	12.824448	-0.055257	4.815549
268.481320	8000.191168	12.829453	-0.055270	4.815552
268.482140	8000.210418	12.834458	-0.055270	4.815558
268.277907	8000.192118	12.839463	-0.055232	4.815553
268.265292	8000.239990	12.844467	-0.055230	4.815567
268.170461	8000.199983	12.849472	-0.055212	4.815556
268.218181	8000.210387	12.854477	-0.055221	4.815559
268.287682	8000.173077	12.859482	-0.055234	4.815548
268.258706	8000.157653	12.864487	-0.055229	4.815543
268.449637	8000.202455	12.869491	-0.055265	4.815556
267.880403	8000.148255	12.874496	-0.055159	4.815542
268.236022	8000.154096	12.879501	-0.055225	4.815542
268.316365	8000.185333	12.884506	-0.055240	4.815551
268.187148	8000.156513	12.889511	-0.055216	4.815543
268.174365	8000.207587	12.894515	-0.055214	4.815558
268.189531	8000.162976	12.899520	-0.055217	4.815545
268.129384	8000.175883	12.904525	-0.055206	4.815549
268.196231	8000.163100	12.909530	-0.055218	4.815545
268.305847	8000.154222	12.914535	-0.055239	4.815542
268.337520	8000.198548	12.919539	-0.055245	4.815555
268.257497	8000.164126	12.924544	-0.055230	4.815545
268.102623	8000.145568	12.929549	-0.055201	4.815541
268.150949	8000.154913	12.934554	-0.055210	4.815543
268.029146	8000.148649	12.939559	-0.055188	4.815542
268.069311	8000.207001	12.944563	-0.055195	4.815559
268.293388	8000.152998	12.949568	-0.055237	4.815542
268.075567	8000.192162	12.954573	-0.055196	4.815554
268.120274	8000.209995	12.959578	-0.055205	4.815559
268.096294	8000.189311	12.964583	-0.055200	4.815553
268.367110	8000.194830	12.969587	-0.055251	4.815554
268.239555	8000.162832	12.974592	-0.055227	4.815545
268.128848	8000.167432	12.979597	-0.055207	4.815547
268.197811	8000.216643	12.984602	-0.055220	4.815561
268.216033	8000.181696	12.989607	-0.055223	4.815551
268.301926	8000.229048	12.994611	-0.055239	4.815564
268.188779	8000.197286	12.999616	-0.055218	4.815555
268.181790	8000.195042	13.004621	-0.055217	4.815555
268.068654	8000.212422	13.009626	-0.055196	4.815560
268.097673	8000.161628	13.014631	-0.055202	4.815545
268.213038	8000.187030	13.019635	-0.055223	4.815552
268.093858	8000.164784	13.024640	-0.055201	4.815546
268.048849	8000.171530	13.029645	-0.055193	4.815548
268.151459	8000.180699	13.034650	-0.055212	4.815551
268.044525	8000.147971	13.039655	-0.055192	4.815542
268.186023	8000.236830	13.044659	-0.055218	4.815567
268.389741	8000.198517	13.049664	-0.055256	4.815555
268.270820	8000.169865	13.054669	-0.055234	4.815547
268.337080	8000.182711	13.059674	-0.055247	4.815550
268.301195	8000.172514	13.064679	-0.055240	4.815547
268.253821	8000.158925	13.069683	-0.055231	4.815544
268.155337	8000.129541	13.074688	-0.055213	4.815536
268.316250	8000.127915	13.079693	-0.055243	4.815534
268.362582	8000.175686	13.084698	-0.055252	4.815548
268.154307	8000.137023	13.089703	-0.055213	4.815538
268.214909	8000.164730	13.094707	-0.055225	4.815546
268.184125	8000.141799	13.099712	-0.055219	4.815539
268.211771	8000.176444	13.104717	-0.055224	4.815549
268.189871	8000.197457	13.109722	-0.055220	4.815555
268.210242	8000.170023	13.114727	-0.055224	4.815547
268.364311	8000.222767	13.119731	-0.055253	4.815562
268.231778	8000.175731	13.124736	-0.055228	4.815549
268.117767	8000.188823	13.129741	-0.055207	4.815553
268.240537	8000.194050	13.134746	-0.055230	4.815554
268.279814	8000.131673	13.139751	-0.055237	4.815536
268.403753	8000.170035	13.144755	-0.055261	4.815546
268.415078	8000.152067	13.149760	-0.055263	4.815541
268.449326	8000.179342	13.154765	-0.055269	4.815549
268.290316	8000.167126	13.159770	-0.055240	4.815546
268.225921	8000.151121	13.164775	-0.055228	4.815542
268.339826	8000.196795	13.169779	-0.055249	4.815554
268.349101	8000.173453	13.174784	-0.055251	4.815547
268.327995	8000.147475	13.179789	-0.055247	4.815540
268.413525	8000.178797	13.184794	-0.055263	4.815549
268.385132	8000.168723	13.189799	-0.055258	4.815546
268.346657	8000.157416	13.194803	-0.055251	4.815543
268.252754	8000.136653	13.199808	-0.055233	4.815537
268.418532	8000.122288	13.204813	-0.055264	4.815532
268.471125	8000.162684	13.209818	-0.055274	4.815544
268.355815	8000.127682	13.214823	-0.055253	4.815534
268.574047	8000.164387	13.219827	-0.055293	4.815544
268.302971	8000.186652	13.224832	-0.055243	4.815552
268.285307	8000.150048	13.229837	-0.055240	4.815541
268.395575	8000.187117	13.234842	-0.055260	4.815551
268.298404	8000.164165	13.239847	-0.055242	4.815545
268.526115	8000.202093	13.244851	-0.055285	4.815555
268.255683	8000.167751	13.249856	-0.055235	4.815546
268.207122	8000.171234	13.254861	-0.055226	4.815547
268.312958	8000.171909	13.259866	-0.055245	4.815547
267.985776	8000.138773	13.264871	-0.055185	4.815539
268.141813	8000.183002	13.269875	-0.055214	4.815551
268.397891	8000.162641	13.274880	-0.055261	4.815544
268.255554	8000.184882	13.279885	-0.055235	4.815551
268.232992	8000.208021	13.284890	-0.055231	4.815558
268.329348	8000.155127	13.289895	-0.055249	4.815542
268.491448	8000.181296	13.294899	-0.055279	4.815549
268.349107	8000.167216	13.299904	-0.055253	4.815546
268.387332	8000.150758	13.304909	-0.055260	4.815541
268.351489	8000.211068	13.309914	-0.055253	4.815558
268.248783	8000.175205	13.314919	-0.055234	4.815548
268.384926	8000.222313	13.319923	-0.055260	4.815562
268.294080	8000.181304	13.324928	-0.055243	4.815550
268.283834	8000.158709	13.329933	-0.055241	4.815543
268.335162	8000.178787	13.334938	-0.055251	4.815549
268.309060	8000.165546	13.339943	-0.055246	4.815545
268.440063	8000.191205	13.344947	-0.055270	4.815552
268.478626	8000.168342	13.349952	-0.055278	4.815545
268.397222	8000.199062	13.354957	-0.055263	4.815555
268.610645	8000.225005	13.359962	-0.055302	4.815561
268.283287	8000.197206	13.364967	-0.055242	4.815555
268.495426	8000.230606	13.369971	-0.055281	4.815563
268.413420	8000.208970	13.374976	-0.055266	4.815557
268.604594	8000.229206	13.379981	-0.055302	4.815562
268.671434	8000.211081	13.384986	-0.055314	4.815557
268.488536	8000.204882	13.389991	-0.055280	4.815556
268.497407	8000.207171	13.394995	-0.055282	4.815557
268.490013	8000.185691	13.400000	-0.055281	4.815550
268.458776	8000.217233	13.405005	-0.055275	4.815560
268.595169	8000.215205	13.410010	-0.055300	4.815558
268.265041	8000.177747	13.415015	-0.055239	4.815549
268.415865	8000.214413	13.420019	-0.055267	4.815559
268.659500	8000.201326	13.425024	-0.055313	4.815554
268.577037	8000.182887	13.430029	-0.055297	4.815549
268.513137	8000.220304	13.435034	-0.055286	4.815560
268.409540	8000.169470	13.440039	-0.055266	4.815546
268.417879	8000.188842	13.445043	-0.055268	4.815552
268.218829	8000.171696	13.450048	-0.055231	4.815547
268.261980	8000.140363	13.455053	-0.055239	4.815538
268.440000	8000.213797	13.460058	-0.055272	4.815559
268.395492	8000.152182	13.465063	-0.055264	4.815541
268.682839	8000.202840	13.470067	-0.055318	4.815554
268.629297	8000.184875	13.475072	-0.055308	4.815549
268.733592	8000.176979	13.480077	-0.055327	4.815547
268.656084	8000.194943	13.485082	-0.055313	4.815552
268.456600	8000.204496	13.490087	-0.055276	4.815556
268.678877	8000.215629	13.495091	-0.055317	4.815558
268.321482	8000.169176	13.500096	-0.055251	4.815546
268.203324	8000.161903	13.505101	-0.055229	4.815545
268.411212	8000.197369	13.510106	-0.055268	4.815554
268.428308	8000.147448	13.515111	-0.055271	4.815539
268.236388	8000.204129	13.520115	-0.055235	4.815557
268.467478	8000.174811	13.525120	-0.055278	4.815547
268.530430	8000.189739	13.530125	-0.055290	4.815551
268.518014	8000.210908	13.535130	-0.055288	4.815557
268.172000	8000.153960	13.540135	-0.055224	4.815542
268.514419	8000.165995	13.545139	-0.055287	4.815544
268.487651	8000.140992	13.550144	-0.055283	4.815537
268.502969	8000.119885	13.555149	-0.055285	4.815531
268.641997	8000.188406	13.560154	-0.055311	4.815550
268.359196	8000.162407	13.565159	-0.055259	4.815544
268.562933	8000.208488	13.570163	-0.055297	4.815557
268.447223	8000.183094	13.575168	-0.055275	4.815550
268.506182	8000.201161	13.580173	-0.055286	4.815555
268.494499	8000.214864	13.585178	-0.055284	4.815559
268.194767	8000.205679	13.590183	-0.055229	4.815557
268.483341	8000.220036	13.595187	-0.055282	4.815560
268.567131	8000.172277	13.600192	-0.055298	4.815546
268.261542	8000.174748	13.605197	-0.055241	4.815548
268.398055	8000.190882	13.610202	-0.055267	4.815552
268.411771	8000.140905	13.615207	-0.055269	4.815537
268.538326	8000.180378	13.620211	-0.055293	4.815548
268.384076	8000.147943	13.625216	-0.055264	4.815540
268.388942	8000.164054	13.630221	-0.055265	4.815544
268.564349	8000.168007	13.635226	-0.055298	4.815545
268.582669	8000.150154	13.640231	-0.055302	4.815539
268.681197	8000.188099	13.645235	-0.055320	4.815550
268.491331	8000.174307	13.650240	-0.055285	4.815547
268.535324	8000.194265	13.655245	-0.055293	4.815552
268.570642	8000.192715	13.660250	-0.055300	4.815552
268.565377	8000.169134	13.665255	-0.055299	4.815545
268.452327	8000.176900	13.670259	-0.055278	4.815548
268.459488	8000.173820	13.675264	-0.055279	4.815547
268.433704	8000.189428	13.680269	-0.055275	4.815552
268.499605	8000.192652	13.685274	-0.055287	4.815552
268.462870	8000.178169	13.690279	-0.055280	4.815548
268.541974	8000.211522	13.695283	-0.055295	4.815557
268.679879	8000.204178	13.700288	-0.055321	4.815555
268.432234	8000.156322	13.705293	-0.055275	4.815542
268.406435	8000.198636	13.710298	-0.055270	4.815554
268.478630	8000.140004	13.715303	-0.055283	4.815537
268.433839	8000.174529	13.720307	-0.055275	4.815547
268.516940	8000.151329	13.725312	-0.055291	4.815540
268.665821	8000.189033	13.730317	-0.055319	4.815550
268.642061	8000.195059	13.735322	-0.055314	4.815552
268.613613	8000.178575	13.740327	-0.055309	4.815547
268.501768	8000.238707	13.745331	-0.055288	4.815566
268.421506	8000.190393	13.750336	-0.055273	4.815552
268.411597	8000.198783	13.755341	-0.055272	4.815554
268.574408	8000.223896	13.760346	-0.055302	4.815561
268.437163	8000.175714	13.765351	-0.055277	4.815547
268.375811	8000.211036	13.770355	-0.055265	4.815558
268.370352	8000.220568	13.775360	-0.055264	4.815561
268.386547	8000.218704	13.780365	-0.055267	4.815560
268.597518	8000.248880	13.785370	-0.055307	4.815568
268.324630	8000.197405	13.790375	-0.055256	4.815554
268.612737	8000.195730	13.795379	-0.055310	4.815552
268.591103	8000.170811	13.800384	-0.055306	4.815545
268.427063	8000.195901	13.805389	-0.055275	4.815553
268.590165	8000.190039	13.810394	-0.055306	4.815551
268.527354	8000.125986	13.815399	-0.055294	4.815532
268.584845	8000.158985	13.820403	-0.055305	4.815542
268.591631	8000.165513	13.825408	-0.055306	4.815544
268.743589	8000.207540	13.830413	-0.055335	4.815555
268.613463	8000.221436	13.835418	-0.055310	4.815560
268.390192	8000.178252	13.840423	-0.055269	4.815548
268.471736	8000.210577	13.845427	-0.055284	4.815557
268.606217	8000.208518	13.850432	-0.055309	4.815556
268.704059	8000.165263	13.855437	-0.055328	4.815543
268.640776	8000.183460	13.860442	-0.055316	4.815549
268.675319	8000.156259	13.865447	-0.055322	4.815541
268.742381	8000.164844	13.870451	-0.055335	4.815543
268.570063	8000.159887	13.875456	-0.055303	4.815542
268.480886	8000.143475	13.880461	-0.055286	4.815538
268.479315	8000.149865	13.885466	-0.055286	4.815540
268.430216	8000.142657	13.890471	-0.055277	4.815538
268.524664	8000.193354	13.895475	-0.055295	4.815552
268.514081	8000.184641	13.900480	-0.055293	4.815550
268.593945	8000.165662	13.905485	-0.055308	4.815544
268.567064	8000.187661	13.910490	-0.055303	4.815550
268.714800	8000.155908	13.915495	-0.055331	4.815540
268.698990	8000.181294	13.920499	-0.055328	4.815548
268.524235	8000.168819	13.925504	-0.055295	4.815545
268.624039	8000.179009	13.930509	-0.055314	4.815547
268.747670	8000.237664	13.935514	-0.055337	4.815564
268.638917	8000.163243	13.940519	-0.055317	4.815543
268.497638	8000.174819	13.945523	-0.055291	4.815547
268.567203	8000.171695	13.950528	-0.055304	4.815546
268.659963	8000.195658	13.955533	-0.055321	4.815552
268.544058	8000.188421	13.960538	-0.055299	4.815551
268.678363	8000.176745	13.965543	-0.055325	4.815547
268.741076	8000.200215	13.970547	-0.055336	4.815553
268.774713	8000.199705	13.975552	-0.055343	4.815553
268.467216	8000.186120	13.980557	-0.055285	4.815550
268.630374	8000.216579	13.985562	-0.055316	4.815558
268.418091	8000.170372	13.990567	-0.055276	4.815546
268.549488	8000.121257	13.995571	-0.055301	4.815531
268.650500	8000.160312	14.000576	-0.055320	4.815542
268.644888	8000.168773	14.005581	-0.055319	4.815544
268.661146	8000.186139	14.010586	-0.055322	4.815549
268.464719	8000.130577	14.015591	-0.055286	4.815534
268.673430	8000.177808	14.020595	-0.055325	4.815547
268.317120	8000.158081	14.025600	-0.055258	4.815543
268.417047	8000.095631	14.030605	-0.055277	4.815524
268.881870	8000.181250	14.035610	-0.055364	4.815547
268.636549	8000.165479	14.040615	-0.055318	4.815543
268.660318	8000.170150	14.045619	-0.055322	4.815545
268.600212	8000.178785	14.050624	-0.055311	4.815547
268.513655	8000.162415	14.055629	-0.055295	4.815543
268.557626	8000.211216	14.060634	-0.055304	4.815557
268.487913	8000.127822	14.065639	-0.055291	4.815533
268.674862	8000.157603	14.070643	-0.055326	4.815541
268.443994	8000.174119	14.075648	-0.055283	4.815547
268.434691	8000.129106	14.080653	-0.055281	4.815534
268.592899	8000.189396	14.085658	-0.055311	4.815551
268.344254	8000.165025	14.090663	-0.055264	4.815545
268.361725	8000.142885	14.095667	-0.055268	4.815538
268.700211	8000.163402	14.100672	-0.055331	4.815542
268.703135	8000.165594	14.105677	-0.055331	4.815543
268.630350	8000.211411	14.110682	-0.055318	4.815557
268.516470	8000.164681	14.115687	-0.055297	4.815544
268.590406	8000.147741	14.120691	-0.055311	4.815538
268.610264	8000.132049	14.125696	-0.055314	4.815534
268.568361	8000.127095	14.130701	-0.055307	4.815532
268.587231	8000.124207	14.135706	-0.055310	4.815532
268.634196	8000.155965	14.140711	-0.055319	4.815541
268.508254	8000.201978	14.145715	-0.055296	4.815555
268.473914	8000.176851	14.150720	-0.055289	4.815547
268.358511	8000.101253	14.155725	-0.055268	4.815526
268.519503	8000.196842	14.160730	-0.055298	4.815553
268.614927	8000.148205	14.165735	-0.055316	4.815538
268.420795	8000.163187	14.170739	-0.055280	4.815544
268.579672	8000.174348	14.175744	-0.055309	4.815546
268.453977	8000.127424	14.180749	-0.055286	4.815533
268.651962	8000.155250	14.185754	-0.055323	4.815540
268.763479	8000.142131	14.190759	-0.055344	4.815536
268.492212	8000.151574	14.195763	-0.055294	4.815540
268.706631	8000.162578	14.200768	-0.055334	4.815542
268.517782	8000.172305	14.205773	-0.055298	4.815546
268.639838	8000.232002	14.210778	-0.055321	4.815563
268.572255	8000.168940	14.215783	-0.055309	4.815545
268.646696	8000.164827	14.220787	-0.055323	4.815543
268.461845	8000.170347	14.225792	-0.055288	4.815546
268.537064	8000.130993	14.230797	-0.055302	4.815534
268.612280	8000.167488	14.235802	-0.055317	4.815544
268.497502	7999.172143	14.240807	-0.055295	4.815254

268.584775	7996.018376	14.245811	-0.055309	4.814331
268.555218	7990.607190	14.250816	-0.055300	4.812750
268.532798	7983.935336	14.255821	-0.055291	4.810798
268.643571	7976.649587	14.260826	-0.055307	4.808666
268.330231	7968.963748	14.265831	-0.055244	4.806417
268.484559	7961.180156	14.270835	-0.055268	4.804137
268.291514	7953.406621	14.275840	-0.055227	4.801860
268.174565	7945.336688	14.280845	-0.055200	4.799495
268.381486	7937.489509	14.285850	-0.055233	4.797193
268.209589	7929.414962	14.290855	-0.055196	4.794824
268.190221	7921.422174	14.295859	-0.055188	4.792477
268.181305	7913.369709	14.300864	-0.055181	4.790112
268.064879	7905.397249	14.305869	-0.055154	4.787770
268.186068	7897.388526	14.310874	-0.055171	4.785415
267.948939	7889.380912	14.315879	-0.055122	4.783060
267.891175	7881.407341	14.320883	-0.055106	4.780713
267.706982	7873.469948	14.325888	-0.055067	4.778377
267.790045	7865.395942	14.330893	-0.055077	4.775998
267.757391	7857.366794	14.335898	-0.055066	4.773631
267.709406	7849.376381	14.340903	-0.055052	4.771275
267.861238	7841.377642	14.345907	-0.055075	4.768915
267.578393	7833.392240	14.350912	-0.055017	4.766559
267.585057	7825.282324	14.355917	-0.055013	4.764163
267.808313	7817.446333	14.360922	-0.055050	4.761847
267.516139	7809.356722	14.365927	-0.054990	4.759457
267.568848	7801.399816	14.370931	-0.054995	4.757103
267.630133	7793.402635	14.375936	-0.055001	4.754736
267.370432	7785.324650	14.380941	-0.054948	4.752345
267.192552	7777.334978	14.385946	-0.054909	4.749979
267.119108	7769.290466	14.390951	-0.054890	4.747595
267.061483	7761.284935	14.395955	-0.054875	4.745222
267.177742	7753.374681	14.400960	-0.054891	4.742874
266.949576	7745.298635	14.405965	-0.054843	4.740478
266.840161	7737.374052	14.410970	-0.054818	4.738125
266.873812	7729.285737	14.415975	-0.054819	4.735722
266.791257	7721.336895	14.420979	-0.054799	4.733359
267.097958	7713.312841	14.425984	-0.054851	4.730971
266.749687	7705.262533	14.430989	-0.054781	4.728577
266.739161	7697.310716	14.435994	-0.054773	4.726209
266.551358	7689.304740	14.440999	-0.054733	4.723825
266.666112	7681.330649	14.446003	-0.054750	4.721448
266.671965	7673.332397	14.451008	-0.054746	4.719064
266.875762	7665.352393	14.456013	-0.054778	4.716682
266.878529	7657.307793	14.461018	-0.054774	4.714281
266.452793	7649.301535	14.466023	-0.054689	4.711891
266.626916	7641.259222	14.471027	-0.054717	4.709488
266.756272	7633.319809	14.476032	-0.054736	4.707114
266.360316	7625.278237	14.481037	-0.054657	4.704710
266.349570	7617.359464	14.486042	-0.054650	4.702341
266.305451	7609.297469	14.491047	-0.054636	4.699927
266.200569	7601.335091	14.496051	-0.054612	4.697542
266.025915	7593.277412	14.501056	-0.054574	4.695127
266.094947	7585.252568	14.506061	-0.054582	4.692721
266.355954	7577.281903	14.511066	-0.054625	4.690329
266.119736	7569.275846	14.516071	-0.054576	4.687927
265.961203	7561.275482	14.521075	-0.054541	4.685524
265.986466	7553.315635	14.526080	-0.054541	4.683132
266.078098	7545.308300	14.531085	-0.054553	4.680725
265.970107	7537.298831	14.536090	-0.054528	4.678316
266.077521	7529.281133	14.541095	-0.054542	4.675903
266.103013	7521.218425	14.546099	-0.054542	4.673475
266.006879	7513.182137	14.551104	-0.054519	4.671055
265.869599	7505.187159	14.556109	-0.054488	4.668645
265.752944	7497.213016	14.561114	-0.054461	4.666241
265.604523	7489.197393	14.566119	-0.054429	4.663822
265.596741	7481.270280	14.571123	-0.054422	4.661429
265.576785	7473.228365	14.576128	-0.054413	4.659000
265.486159	7465.264781	14.581133	-0.054391	4.656594
265.488062	7457.212751	14.586138	-0.054386	4.654159
265.183293	7449.218685	14.591143	-0.054325	4.651741
265.259338	7441.188746	14.596147	-0.054334	4.649311
265.269077	7433.285460	14.601152	-0.054330	4.646917
265.159792	7425.189194	14.606157	-0.054305	4.644465
265.425305	7417.300948	14.611162	-0.054349	4.642073
265.288970	7409.230596	14.616167	-0.054319	4.639625
265.169152	7401.246877	14.621171	-0.054291	4.637203
265.348149	7393.233973	14.626176	-0.054319	4.634770
265.140845	7385.185587	14.631181	-0.054276	4.632325
265.182248	7377.195266	14.636186	-0.054278	4.629896
265.214978	7369.190645	14.641191	-0.054279	4.627462
264.878467	7361.178603	14.646195	-0.054211	4.625024
264.737154	7353.205928	14.651200	-0.054180	4.622597
264.681726	7345.141225	14.656205	-0.054164	4.620141
264.777073	7337.195603	14.661210	-0.054177	4.617720
264.840809	7329.179388	14.666215	-0.054184	4.615275
264.736774	7321.184803	14.671219	-0.054159	4.612836
264.641100	7313.151544	14.676224	-0.054136	4.610384
264.744263	7305.158292	14.681229	-0.054150	4.607943
264.733932	7297.173399	14.686234	-0.054143	4.605503
264.608553	7289.198968	14.691239	-0.054115	4.603066
264.612157	7281.162365	14.696243	-0.054110	4.600607
264.547322	7273.195416	14.701248	-0.054093	4.598169
264.423346	7265.164515	14.706253	-0.054065	4.595710
264.470929	7257.115286	14.711258	-0.054069	4.593244
264.321934	7249.076829	14.716263	-0.054036	4.590780
264.179919	7241.109904	14.721267	-0.054004	4.588336
264.173070	7233.148010	14.726272	-0.053998	4.585893
264.115122	7225.122383	14.731277	-0.053982	4.583428
264.148907	7217.145572	14.736282	-0.053983	4.580978
264.159486	7209.107084	14.741287	-0.053980	4.578507
264.158610	7201.145031	14.746291	-0.053975	4.576059
263.932477	7193.094633	14.751296	-0.053927	4.573581
263.712365	7185.067936	14.756301	-0.053881	4.571110
263.898741	7177.132395	14.761306	-0.053911	4.568666
263.823138	7169.143273	14.766311	-0.053892	4.566203
263.653119	7161.101173	14.771315	-0.053855	4.563723
263.683248	7153.188138	14.776320	-0.053855	4.561282
263.627769	7145.138155	14.781325	-0.053840	4.558797
263.555694	7137.166433	14.786330	-0.053821	4.556334
263.741194	7129.122103	14.791335	-0.053851	4.553849
263.779577	7121.088875	14.796339	-0.053853	4.551365
263.579539	7113.090492	14.801344	-0.053810	4.548890
263.360755	7105.125887	14.806349	-0.053764	4.546424
263.456238	7097.118632	14.811354	-0.053777	4.543944
263.394179	7089.129703	14.816359	-0.053760	4.541469
263.443624	7081.102232	14.821363	-0.053764	4.538980
263.222510	7073.137129	14.826368	-0.053718	4.536508
263.061913	7065.097651	14.831373	-0.053683	4.534013
262.994447	7057.089206	14.836378	-0.053665	4.531525
262.980177	7049.091872	14.841383	-0.053657	4.529040
263.090331	7041.107128	14.846387	-0.053673	4.526558
263.240918	7033.112399	14.851392	-0.053696	4.524071
263.093927	7025.145216	14.856397	-0.053663	4.521591
263.125242	7017.087945	14.861402	-0.053664	4.519082
263.110169	7009.162708	14.866407	-0.053656	4.516613
262.853680	7001.102542	14.871411	-0.053603	4.514099
262.920448	6993.028387	14.876416	-0.053610	4.511581
262.759194	6985.004586	14.881421	-0.053575	4.509076
262.884239	6977.061873	14.886426	-0.053593	4.506596
262.479982	6969.034129	14.891431	-0.053513	4.504086
262.666344	6961.087717	14.896435	-0.053543	4.501602
262.735233	6953.088807	14.901440	-0.053550	4.499100
262.449010	6945.080621	14.906445	-0.053492	4.496593
262.505980	6937.088768	14.911450	-0.053497	4.494090
262.465105	6929.050488	14.916455	-0.053485	4.491572
262.413135	6921.045720	14.921459	-0.053470	4.489062
262.558041	6913.042510	14.926464	-0.053492	4.486552
262.410023	6905.016858	14.931469	-0.053459	4.484032
262.456743	6897.079249	14.936474	-0.053462	4.481540
262.210369	6889.040853	14.941479	-0.053411	4.479013
262.417738	6881.095563	14.946483	-0.053445	4.476516
262.288295	6873.047176	14.951488	-0.053416	4.473984
261.811819	6865.024107	14.956493	-0.053322	4.471457
262.004273	6857.028951	14.961498	-0.053352	4.468939
261.888473	6849.034833	14.966503	-0.053326	4.466420
261.946708	6841.003654	14.971507	-0.053331	4.463888
261.861517	6833.066769	14.976512	-0.053311	4.461384
261.807405	6825.000520	14.981517	-0.053295	4.458837
261.914488	6817.039711	14.986522	-0.053310	4.456324
261.700873	6808.975740	14.991527	-0.053265	4.453774
261.621382	6800.967102	14.996531	-0.053245	4.451242
261.741439	6793.004896	15.001536	-0.053262	4.448723
261.707054	6785.013675	15.006541	-0.053251	4.446194
261.742168	6776.978806	15.011546	-0.053252	4.443649
261.677280	6769.034570	15.016551	-0.053235	4.441131
261.539019	6761.035830	15.021555	-0.053204	4.438594
261.405752	6753.039689	15.026560	-0.053174	4.436056
261.366518	6744.988863	15.031565	-0.053162	4.433500
261.440059	6736.955843	15.036570	-0.053170	4.430949
261.169705	6728.964778	15.041575	-0.053115	4.428408
261.282205	6720.938487	15.046579	-0.053131	4.425856
261.401847	6713.004963	15.051584	-0.053148	4.423332
261.166454	6705.002811	15.056589	-0.053099	4.420784
261.028968	6696.992134	15.061594	-0.053068	4.418231
261.035471	6688.965336	15.066599	-0.053064	4.415673
260.960871	6680.959135	15.071603	-0.053045	4.413119
261.122150	6672.986172	15.076608	-0.053070	4.410575
260.973425	6665.005092	15.081613	-0.053037	4.408026
261.011100	6657.002247	15.086618	-0.053039	4.405470
260.883743	6648.994039	15.091623	-0.053010	4.402909
260.647332	6640.975760	15.096627	-0.052961	4.400343
260.944367	6633.018692	15.101632	-0.053011	4.397798
260.806122	6624.977958	15.106637	-0.052980	4.395222
260.939141	6616.972432	15.111642	-0.053000	4.392658
260.769186	6608.941725	15.116647	-0.052963	4.390082
260.785955	6600.938813	15.121651	-0.052961	4.387515
260.593289	6592.929701	15.126656	-0.052920	4.384943
260.606122	6585.003330	15.131661	-0.052918	4.382397
260.746180	6577.015173	15.136666	-0.052939	4.379831
260.471689	6569.015917	15.141671	-0.052882	4.377257
260.457903	6560.947803	15.146675	-0.052875	4.374661
260.378092	6552.993334	15.151680	-0.052855	4.372100
260.275364	6544.947106	15.156685	-0.052830	4.369508
260.240294	6537.016741	15.161690	-0.052819	4.366951
260.336790	6528.952061	15.166695	-0.052831	4.364351
260.414585	6521.043399	15.171699	-0.052841	4.361799
260.156120	6513.008673	15.176704	-0.052788	4.359203
259.890874	6504.995402	15.181709	-0.052733	4.356613
260.183497	6496.973929	15.186714	-0.052782	4.354021
260.073048	6488.888067	15.191719	-0.052757	4.351405
259.867076	6480.878496	15.196723	-0.052713	4.348811
259.997933	6472.921797	15.201728	-0.052732	4.346236
259.735363	6464.929782	15.206733	-0.052678	4.343644
259.679260	6456.968162	15.211738	-0.052663	4.341062
259.709693	6448.945988	15.216743	-0.052663	4.338460
259.524660	6440.941874	15.221747	-0.052624	4.335860
259.680698	6433.006398	15.226752	-0.052648	4.333283
259.620034	6424.895928	15.231757	-0.052631	4.330647
259.498627	6416.939550	15.236762	-0.052603	4.328058
259.175333	6408.938745	15.241767	-0.052538	4.325452
259.113654	6400.968691	15.246771	-0.052522	4.322857
259.210432	6392.943373	15.251776	-0.052534	4.320243
259.063661	6385.003083	15.256781	-0.052502	4.317653
259.094708	6376.932474	15.261786	-0.052503	4.315020
259.217514	6368.925864	15.266791	-0.052520	4.312408
259.272096	6360.890295	15.271795	-0.052525	4.309784
259.280669	6352.953323	15.276800	-0.052522	4.307190
259.017214	6344.907315	15.281805	-0.052468	4.304557
259.147414	6336.959012	15.286810	-0.052487	4.301957
258.940378	6328.886311	15.291815	-0.052443	4.299313
259.001569	6320.976025	15.296819	-0.052449	4.296722
258.895796	6312.916525	15.301824	-0.052424	4.294079
259.096143	6304.911586	15.306829	-0.052457	4.291455
259.099649	6296.903045	15.311834	-0.052452	4.288827
258.807007	6288.917284	15.316839	-0.052393	4.286202
258.997912	6280.900603	15.321843	-0.052423	4.283569
258.878810	6272.951711	15.326848	-0.052396	4.280954
258.739534	6264.920977	15.331853	-0.052365	4.278311
258.900349	6256.952941	15.336858	-0.052389	4.275689
258.702978	6248.918513	15.341863	-0.052347	4.273040
258.593009	6240.852780	15.346867	-0.052322	4.270381
258.647805	6232.883347	15.351872	-0.052327	4.267753
258.482978	6224.854667	15.356877	-0.052291	4.265102
258.429380	6216.903681	15.361882	-0.052276	4.262475
258.267500	6208.923710	15.366887	-0.052241	4.259837
258.265973	6200.885879	15.371891	-0.052235	4.257179
258.394953	6192.911765	15.376896	-0.052254	4.254542
258.138601	6184.864548	15.381901	-0.052201	4.251875
258.070110	6176.894534	15.386906	-0.052183	4.249235
257.984824	6168.887610	15.391911	-0.052162	4.246580
257.707902	6160.916532	15.396915	-0.052106	4.243933
257.928155	6152.943048	15.401920	-0.052142	4.241289
257.809203	6144.966271	15.406925	-0.052114	4.238639
257.754037	6136.931661	15.411930	-0.052099	4.235968
257.810466	6128.929897	15.416935	-0.052104	4.233308
257.912595	6120.872725	15.421939	-0.052118	4.230628
258.048655	6112.918994	15.426944	-0.052138	4.227981
257.833694	6104.880306	15.431949	-0.052093	4.225301
257.995688	6096.964826	15.436954	-0.052118	4.222664
257.861648	6088.919922	15.441959	-0.052088	4.219979
257.841356	6080.959064	15.446963	-0.052079	4.217321
257.617892	6072.939303	15.451968	-0.052032	4.214640
257.486275	6064.921014	15.456973	-0.052003	4.211959
257.473471	6056.908917	15.461978	-0.051995	4.209279
257.279197	6048.947633	15.466983	-0.051954	4.206613
257.119565	6040.931690	15.471987	-0.051919	4.203927
257.041637	6032.955649	15.476992	-0.051899	4.201254
257.128038	6024.938604	15.481997	-0.051910	4.198567
257.110449	6016.998790	15.487002	-0.051902	4.195903
257.112375	6008.887707	15.492007	-0.051897	4.193180
257.027593	6000.804185	15.497011	-0.051876	4.190464
257.019863	5992.861804	15.502016	-0.051870	4.187794
256.917655	5984.846836	15.507021	-0.051846	4.185096
257.004093	5976.908827	15.512026	-0.051857	4.182426
257.000024	5968.878748	15.517031	-0.051851	4.179721
256.915635	5960.914864	15.522035	-0.051830	4.177036
256.854785	5952.910015	15.527040	-0.051813	4.174336
256.862847	5944.872011	15.532045	-0.051810	4.171623
256.801459	5936.878538	15.537050	-0.051793	4.168924
256.573526	5928.900513	15.542055	-0.051746	4.166225
256.575590	5920.899646	15.547059	-0.051741	4.163520
256.473348	5912.916770	15.552064	-0.051717	4.160818
256.490699	5904.897229	15.557069	-0.051715	4.158103
256.569004	5896.925041	15.562074	-0.051724	4.155403
256.430540	5888.924104	15.567079	-0.051693	4.152689
256.213848	5880.841031	15.572083	-0.051648	4.149945
256.217015	5872.891758	15.577088	-0.051643	4.147246
256.170208	5864.856628	15.582093	-0.051629	4.144516
256.299725	5856.916057	15.587098	-0.051648	4.141819
256.268392	5848.876237	15.592103	-0.051637	4.139084
256.215114	5840.923235	15.597107	-0.051622	4.136377
256.176823	5832.887871	15.602112	-0.051610	4.133640
255.945562	5824.842870	15.607117	-0.051562	4.130895
256.376013	5816.844175	15.612122	-0.051637	4.128173
255.982162	5808.897256	15.617127	-0.051558	4.125456
255.813443	5800.932823	15.622131	-0.051522	4.122734
256.016458	5792.921600	15.627136	-0.051555	4.119999
255.671234	5784.914122	15.632141	-0.051485	4.117257
255.922298	5776.902587	15.637146	-0.051527	4.114519
255.893519	5768.843918	15.642151	-0.051516	4.111759
255.722439	5760.797880	15.647155	-0.051479	4.109000
255.644832	5752.894869	15.652160	-0.051460	4.106290
255.325652	5744.878984	15.657165	-0.051395	4.103536
255.447094	5736.895342	15.662170	-0.051413	4.100796
255.361475	5728.908627	15.667175	-0.051391	4.098052
255.296776	5720.895627	15.672179	-0.051374	4.095296
255.562302	5712.898775	15.677184	-0.051419	4.092549
255.295078	5704.889067	15.682189	-0.051364	4.089788
255.111249	5696.937778	15.687194	-0.051324	4.087047
255.278446	5688.905591	15.692199	-0.051350	4.084280
255.318691	5680.931783	15.697203	-0.051353	4.081530
255.423261	5672.948113	15.702208	-0.051367	4.078776
255.335836	5664.945879	15.707213	-0.051346	4.076011
255.331792	5656.938532	15.712218	-0.051340	4.073243
255.205030	5648.873030	15.717223	-0.051311	4.070452
254.988353	5640.905150	15.722227	-0.051266	4.067691
255.240762	5632.913678	15.727232	-0.051307	4.064927
254.989352	5624.914030	15.732237	-0.051255	4.062151
255.001892	5616.944159	15.737242	-0.051253	4.059387
254.771800	5608.984388	15.742247	-0.051205	4.056621
254.854963	5600.941606	15.747251	-0.051215	4.053829
254.824190	5592.951315	15.752256	-0.051204	4.051052
254.841974	5584.905253	15.757261	-0.051202	4.048254
254.645483	5576.918647	15.762266	-0.051161	4.045471
254.553355	5568.950221	15.767271	-0.051138	4.042695
254.417459	5560.919329	15.772275	-0.051108	4.039894
254.656324	5552.980036	15.777280	-0.051147	4.037129
254.361902	5544.933999	15.782285	-0.051087	4.034317
254.368617	5536.824384	15.787290	-0.051083	4.031485
254.304794	5528.837845	15.792295	-0.051066	4.028693
254.306501	5520.834385	15.797299	-0.051061	4.025894
254.316535	5512.906584	15.802304	-0.051058	4.023120
254.194117	5504.894725	15.807309	-0.051030	4.020312
254.133198	5496.954377	15.812314	-0.051014	4.017529
254.122660	5488.908755	15.817319	-0.051007	4.014707
254.018552	5480.904988	15.822323	-0.050982	4.011896
254.134642	5472.893466	15.827328	-0.050999	4.009085
254.068422	5464.895720	15.832333	-0.050981	4.006273
253.951982	5456.920091	15.837338	-0.050954	4.003466
253.982380	5448.930149	15.842343	-0.050955	4.000655
253.957122	5440.920881	15.847347	-0.050945	3.997834
253.923577	5432.929175	15.852352	-0.050934	3.995017
253.794235	5424.882042	15.857357	-0.050905	3.992177
253.831377	5416.851588	15.862362	-0.050906	3.989343
253.664220	5408.927312	15.867367	-0.050870	3.986542
253.425587	5400.892798	15.872371	-0.050820	3.983699
253.531754	5392.946851	15.877376	-0.050835	3.980890
253.579888	5384.942180	15.882381	-0.050839	3.978058
253.387885	5376.945695	15.887386	-0.050798	3.975222
253.235333	5368.920559	15.892391	-0.050765	3.972375
253.179414	5360.876421	15.897395	-0.050749	3.969521
253.236974	5352.955783	15.902400	-0.050755	3.966711
253.368908	5344.930868	15.907405	-0.050774	3.963863
253.336432	5336.970498	15.912410	-0.050763	3.961033
253.366522	5328.986497	15.917415	-0.050763	3.958193
253.148050	5320.985193	15.922419	-0.050718	3.955341
253.119831	5312.976123	15.927424	-0.050707	3.952488
253.021896	5304.885214	15.932429	-0.050684	3.949602
253.269420	5296.949544	15.937434	-0.050725	3.946775
253.081205	5288.978843	15.942439	-0.050685	3.943926
252.850365	5280.955818	15.947443	-0.050636	3.941056
252.782990	5273.010942	15.952448	-0.050619	3.938214
252.571970	5264.983911	15.957453	-0.050574	3.935338
252.711455	5256.995001	15.962458	-0.050595	3.932481
252.565812	5248.986963	15.967463	-0.050563	3.929609
252.342344	5240.998344	15.972467	-0.050516	3.926740
252.269304	5233.002836	15.977472	-0.050497	3.923870
252.470724	5224.975815	15.982477	-0.050530	3.920991
252.589119	5216.994449	15.987482	-0.050547	3.918125
252.555460	5209.012774	15.992487	-0.050535	3.915254
252.377561	5200.968937	15.997491	-0.050497	3.912356
252.476573	5192.971461	16.002496	-0.050510	3.909477
252.217250	5184.994916	16.007501	-0.050457	3.906598
252.365139	5176.962555	16.012506	-0.050479	3.903703
252.336541	5168.994577	16.017511	-0.050469	3.900827
251.976721	5161.017860	16.022515	-0.050397	3.897938
252.272640	5153.012777	16.027520	-0.050447	3.895050
252.247702	5144.979527	16.032525	-0.050437	3.892144
252.049488	5136.939049	16.037530	-0.050395	3.889229
251.962568	5129.002147	16.042535	-0.050374	3.886352
252.058342	5120.964166	16.047539	-0.050386	3.883439
252.097839	5113.016900	16.052544	-0.050388	3.880556
251.701261	5104.995802	16.057549	-0.050309	3.877636
251.923114	5097.006866	16.062554	-0.050346	3.874737
251.818138	5088.772030	16.067559	-0.050321	3.871740
251.759652	5080.810349	16.072563	-0.050305	3.868842
251.584039	5072.914171	16.077568	-0.050267	3.865962
251.470549	5064.918672	16.082573	-0.050241	3.863046
251.454015	5056.976995	16.087578	-0.050233	3.860148
251.406711	5048.956640	16.092583	-0.050219	3.857220
251.280877	5040.977495	16.097587	-0.050190	3.854302
251.511043	5033.008623	16.102592	-0.050228	3.851393
251.147700	5024.975477	16.107597	-0.050155	3.848447
251.041638	5016.991393	16.112602	-0.050130	3.845521
251.081570	5009.017185	16.117607	-0.050132	3.842600
251.142244	5000.984890	16.122611	-0.050139	3.839656
250.955109	4993.087507	16.127616	-0.050099	3.836753
250.854836	4985.043423	16.132621	-0.050075	3.833797
250.908406	4977.035067	16.137626	-0.050080	3.830854
250.858303	4969.020937	16.142631	-0.050065	3.827905
250.625601	4961.020906	16.147635	-0.050017	3.824955
250.791424	4953.104251	16.152640	-0.050043	3.822042
250.767781	4945.037724	16.157645	-0.050033	3.819068
250.498458	4937.088947	16.162650	-0.049978	3.816129
250.678772	4929.073885	16.167655	-0.050006	3.813173
250.699670	4921.043832	16.172659	-0.050005	3.810206
250.752433	4913.078927	16.177664	-0.050010	3.807261
250.548750	4905.036527	16.182669	-0.049967	3.804280
250.435889	4897.123249	16.187674	-0.049940	3.801346
250.242765	4889.103008	16.192679	-0.049899	3.798369
250.252243	4881.079696	16.197683	-0.049896	3.795392
250.448915	4873.084361	16.202688	-0.049927	3.792428
250.239911	4865.027788	16.207693	-0.049883	3.789429
250.136264	4857.056996	16.212698	-0.049859	3.786463
250.088602	4849.071541	16.217703	-0.049845	3.783490
250.046360	4841.064415	16.222707	-0.049832	3.780506
250.197785	4833.099685	16.227712	-0.049855	3.777541
249.997374	4825.072910	16.232717	-0.049813	3.774542
250.020561	4817.085021	16.237722	-0.049812	3.771560
249.829125	4809.106479	16.242727	-0.049771	3.768574
249.648099	4801.065283	16.247731	-0.049732	3.765563
249.729065	4793.156320	16.252736	-0.049742	3.762605
249.559992	4785.090599	16.257741	-0.049705	3.759580
249.898261	4777.126737	16.262746	-0.049763	3.756603
249.783348	4769.118860	16.267751	-0.049737	3.753596
249.664111	4761.058709	16.272755	-0.049709	3.750567
249.472745	4753.135023	16.277760	-0.049669	3.747585
249.532995	4745.089174	16.282765	-0.049675	3.744561
249.602571	4737.148725	16.287770	-0.049683	3.741574
249.333866	4729.143031	16.292775	-0.049627	3.738552
249.260268	4721.134961	16.297779	-0.049609	3.735532
249.278545	4713.142492	16.302784	-0.049607	3.732517
249.101118	4705.098625	16.307789	-0.049569	3.729475
249.054871	4697.165380	16.312794	-0.049555	3.726476
249.238510	4689.158707	16.317799	-0.049584	3.723453
249.250380	4681.155429	16.322803	-0.049581	3.720424
249.219424	4673.217436	16.327808	-0.049570	3.717416
249.014086	4665.176099	16.332813	-0.049527	3.714362
248.867278	4657.096573	16.337818	-0.049494	3.711293
248.809884	4649.122383	16.342823	-0.049478	3.708264
248.929028	4641.084162	16.347827	-0.049496	3.705212
248.877046	4633.180160	16.352832	-0.049481	3.702204
248.646630	4625.163096	16.357837	-0.049433	3.699146
248.509376	4617.243321	16.362842	-0.049402	3.696125
248.647650	4609.181045	16.367847	-0.049423	3.693054
248.654322	4601.151261	16.372851	-0.049419	3.689990
248.636791	4593.209820	16.377856	-0.049410	3.686957
248.460206	4585.202196	16.382861	-0.049372	3.683891
248.571997	4577.228654	16.387866	-0.049388	3.680843
248.458014	4569.269383	16.392871	-0.049362	3.677793
248.325386	4561.210526	16.397875	-0.049332	3.674701
248.496247	4553.224420	16.402880	-0.049359	3.671643
248.192648	4545.232893	16.407885	-0.049297	3.668567
248.211932	4537.192325	16.412890	-0.049295	3.665478
248.283075	4529.223199	16.417895	-0.049303	3.662416
248.305718	4521.218590	16.422899	-0.049303	3.659336
248.239216	4513.271340	16.427904	-0.049285	3.656274
247.983874	4505.235181	16.432909	-0.049232	3.653169
247.894867	4497.228571	16.437914	-0.049211	3.650078
247.912512	4489.259459	16.442919	-0.049209	3.647001
247.761915	4481.252116	16.447923	-0.049176	3.643902
247.651547	4473.300518	16.452928	-0.049150	3.640824
247.602747	4465.273249	16.457933	-0.049136	3.637715
247.690529	4457.273200	16.462938	-0.049147	3.634617
247.416863	4449.255179	16.467943	-0.049091	3.631501
247.330611	4441.239945	16.472947	-0.049070	3.628387
247.452459	4433.252428	16.477952	-0.049087	3.625288
247.321542	4425.288616	16.482957	-0.049058	3.622188
247.418576	4417.272351	16.487962	-0.049071	3.619071
247.589891	4409.298581	16.492967	-0.049097	3.615971
247.515322	4401.276111	16.497971	-0.049078	3.612841
247.372024	4393.279101	16.502976	-0.049047	3.609718
247.387872	4385.292156	16.507981	-0.049044	3.606599
247.396723	4377.313414	16.512986	-0.049041	3.603481
247.198612	4369.355574	16.517991	-0.048999	3.600363
247.122121	4361.365716	16.522995	-0.048980	3.597233
247.093653	4353.375419	16.528000	-0.048969	3.594101
246.913378	4345.344161	16.533005	-0.048930	3.590947
246.690274	4337.363687	16.538010	-0.048884	3.587808
246.881667	4329.357098	16.543015	-0.048914	3.584668
246.607249	4321.396835	16.548019	-0.048858	3.581530
246.694895	4313.398278	16.553024	-0.048869	3.578384
246.613751	4305.405577	16.558029	-0.048849	3.575233
246.572547	4297.401209	16.563034	-0.048836	3.572077
246.657628	4289.379646	16.568039	-0.048847	3.568914
246.467912	4281.388548	16.573043	-0.048806	3.565752
246.526573	4273.452609	16.578048	-0.048812	3.562617
246.415771	4265.422599	16.583053	-0.048786	3.559436
246.407146	4257.459222	16.588058	-0.048780	3.556282
246.469727	4249.376378	16.593063	-0.048786	3.553080
246.450685	4241.320256	16.598067	-0.048777	3.549884
246.188024	4233.421647	16.603072	-0.048723	3.546740
246.265977	4225.370368	16.608077	-0.048733	3.543542
246.313161	4217.382767	16.613082	-0.048736	3.540366
246.122004	4209.436735	16.618087	-0.048696	3.537197
246.201437	4201.411699	16.623091	-0.048705	3.534001
246.104438	4193.450282	16.628096	-0.048682	3.530822
245.870342	4185.451777	16.633101	-0.048634	3.527622
245.784314	4177.432192	16.638106	-0.048612	3.524415
245.910127	4169.487269	16.643111	-0.048631	3.521241
245.614683	4161.493600	16.648115	-0.048571	3.518032
245.665789	4153.508043	16.653120	-0.048575	3.514834
245.869622	4145.450300	16.658125	-0.048608	3.511608
245.796838	4137.471723	16.663130	-0.048589	3.508403
245.586771	4129.501764	16.668135	-0.048545	3.505194
245.615927	4121.507481	16.673139	-0.048545	3.501980
245.820548	4113.523957	16.678144	-0.048578	3.498773
245.454882	4105.563408	16.683149	-0.048505	3.495554
245.392971	4097.547192	16.688154	-0.048488	3.492320
245.368839	4089.553262	16.693159	-0.048479	3.489092
245.137750	4081.571392	16.698163	-0.048430	3.485860
245.176515	4073.593565	16.703168	-0.048433	3.482635
245.070541	4065.576706	16.708173	-0.048408	3.479386
245.072296	4057.626652	16.713178	-0.048403	3.476165
245.075368	4049.569983	16.718183	-0.048398	3.472898
245.022595	4041.547627	16.723187	-0.048383	3.469640
245.053236	4033.600696	16.728192	-0.048384	3.466412
244.826243	4025.578894	16.733197	-0.048337	3.463143
244.851368	4017.605940	16.738202	-0.048336	3.459898
244.896768	4009.618919	16.743207	-0.048339	3.456645
245.001572	4001.591014	16.748211	-0.048354	3.453375
244.561192	3993.636760	16.753216	-0.048267	3.450113
244.849996	3985.606147	16.758221	-0.048315	3.446841
244.690403	3977.631536	16.763226	-0.048280	3.443574
244.390305	3969.672924	16.768231	-0.048219	3.440306
244.285537	3961.685570	16.773235	-0.048195	3.437030
244.278723	3953.698660	16.778240	-0.048188	3.433753
244.226632	3945.653916	16.783245	-0.048174	3.430449
244.176588	3937.667660	16.788250	-0.048159	3.427165
244.299142	3929.665811	16.793255	-0.048177	3.423878
244.206039	3921.691617	16.798259	-0.048154	3.420591
244.204280	3913.742586	16.803264	-0.048149	3.417315
244.175202	3905.702084	16.808269	-0.048138	3.413997
244.195952	3897.684179	16.813274	-0.048137	3.410686
244.108884	3889.737364	16.818279	-0.048116	3.407399
243.847943	3881.721487	16.823283	-0.048062	3.404073
244.036218	3873.767243	16.828288	-0.048092	3.400785
243.986031	3865.777329	16.833293	-0.048077	3.397471
243.961888	3857.793806	16.838298	-0.048068	3.394158
244.011508	3849.693951	16.843303	-0.048072	3.390795
243.705008	3841.715416	16.848307	-0.048010	3.387467
243.626701	3833.765341	16.853312	-0.047990	3.384155
243.579319	3825.789762	16.858317	-0.047976	3.380831
243.576358	3817.810055	16.863322	-0.047970	3.377503
243.573887	3809.824721	16.868327	-0.047965	3.374170
243.416537	3801.808203	16.873331	-0.047930	3.370815
243.278019	3793.830218	16.878336	-0.047899	3.367473
243.320261	3785.824627	16.883341	-0.047902	3.364123
243.379532	3777.871698	16.888346	-0.047908	3.360792
243.361759	3769.872260	16.893351	-0.047900	3.357435
243.088564	3761.869404	16.898355	-0.047844	3.354065
243.259775	3753.835604	16.903360	-0.047870	3.350694
243.029604	3745.860869	16.908365	-0.047822	3.347330
243.238441	3737.855439	16.913370	-0.047856	3.343966
243.011849	3729.906189	16.918375	-0.047809	3.340606
242.956888	3721.910169	16.923379	-0.047794	3.337229
243.016948	3713.918874	16.928384	-0.047800	3.333855
243.031771	3705.902712	16.933389	-0.047797	3.330466
242.787028	3697.944747	16.938394	-0.047747	3.327088
242.653759	3689.941743	16.943399	-0.047717	3.323691
242.861056	3681.941991	16.948403	-0.047750	3.320305
242.758638	3674.001900	16.953408	-0.047726	3.316930
242.429892	3665.987201	16.958413	-0.047659	3.313511
242.487316	3657.948157	16.963418	-0.047665	3.310092
242.573009	3649.968358	16.968423	-0.047676	3.306696
242.488123	3641.981908	16.973427	-0.047655	3.303288
242.536910	3634.015209	16.978432	-0.047659	3.299889
242.563335	3626.022913	16.983437	-0.047659	3.296475
242.223615	3618.052015	16.988442	-0.047590	3.293053
242.270316	3610.052666	16.993447	-0.047594	3.289630
242.023210	3602.073519	16.998451	-0.047543	3.286200
242.194939	3594.078851	17.003456	-0.047570	3.282776
241.863578	3586.107421	17.008461	-0.047503	3.279340
241.912954	3578.129606	17.013466	-0.047507	3.275911
241.946290	3570.101406	17.018471	-0.047508	3.272457
241.691769	3562.092659	17.023475	-0.047455	3.268997
241.758731	3554.120351	17.028480	-0.047463	3.265560
241.670934	3546.127190	17.033485	-0.047441	3.262106
241.697475	3538.146509	17.038490	-0.047441	3.258657
241.569760	3530.173280	17.043495	-0.047412	3.255202
241.638022	3522.136532	17.048499	-0.047420	3.251723
241.720368	3514.155268	17.053504	-0.047430	3.248266
241.449506	3506.166926	17.058509	-0.047374	3.244787
241.470201	3498.224925	17.063514	-0.047373	3.241337
241.505968	3490.235465	17.068519	-0.047375	3.237863
241.145282	3482.236955	17.073523	-0.047302	3.234365
241.294263	3474.176910	17.078528	-0.047325	3.230857
241.436202	3466.175538	17.083533	-0.047346	3.227371
241.366122	3458.210429	17.088538	-0.047328	3.223888
241.368861	3450.233587	17.093543	-0.047323	3.220399
241.178871	3442.268522	17.098547	-0.047283	3.216903
241.226831	3434.283416	17.103552	-0.047287	3.213405
240.941412	3426.270155	17.108557	-0.047228	3.209877
240.759038	3418.292336	17.113562	-0.047189	3.206365
240.948639	3410.318644	17.118567	-0.047220	3.202866
240.780680	3402.331506	17.123571	-0.047183	3.199342
240.655253	3394.386023	17.128576	-0.047155	3.195835
240.525686	3386.350719	17.133581	-0.047125	3.192284
240.544093	3378.343499	17.138586	-0.047124	3.188748
240.505901	3370.369619	17.143591	-0.047111	3.185220
240.543665	3362.363486	17.148595	-0.047113	3.181677
240.609324	3354.396665	17.153600	-0.047121	3.178149
240.397727	3346.414705	17.158605	-0.047076	3.174598
240.357505	3338.406998	17.163610	-0.047063	3.171040
240.292819	3330.427505	17.168615	-0.047046	3.167488
240.190701	3322.424176	17.173619	-0.047022	3.163921
240.168343	3314.469795	17.178624	-0.047013	3.160375
240.083381	3306.512259	17.183629	-0.046992	3.156820
240.222866	3298.455961	17.188634	-0.047013	3.153227
240.174634	3290.453606	17.193639	-0.046999	3.149646
239.877345	3282.500755	17.198643	-0.046938	3.146073
239.893246	3274.536159	17.203648	-0.046936	3.142503
239.996154	3266.510879	17.208653	-0.046950	3.138906
239.860496	3258.546686	17.213658	-0.046920	3.135322
239.943506	3250.547925	17.218663	-0.046930	3.131728
239.501642	3242.576174	17.223667	-0.046842	3.128119
239.463826	3234.599487	17.228672	-0.046830	3.124521
239.655957	3226.614057	17.233677	-0.046861	3.120926
239.380544	3218.638593	17.238682	-0.046805	3.117309
239.429465	3210.656116	17.243687	-0.046809	3.113700
239.378858	3202.621149	17.248691	-0.046794	3.110059
239.501007	3194.652678	17.253696	-0.046812	3.106451
239.246478	3186.676120	17.258701	-0.046759	3.102818
239.269272	3178.688091	17.263706	-0.046758	3.099189
239.393554	3170.716357	17.268711	-0.046776	3.095567
239.270142	3162.681573	17.273715	-0.046748	3.091901
239.160178	3154.711805	17.278720	-0.046723	3.088260
239.162940	3146.713453	17.283725	-0.046718	3.084608
239.176438	3138.761706	17.288730	-0.046715	3.080973
239.164532	3130.807601	17.293735	-0.046708	3.077331
238.957065	3122.798371	17.298739	-0.046664	3.073651
238.868453	3114.738460	17.303744	-0.046643	3.069949
238.794973	3106.749260	17.308749	-0.046624	3.066275
238.792556	3098.771230	17.313754	-0.046618	3.062606
238.936523	3090.818942	17.318759	-0.046640	3.058950
238.723262	3082.848447	17.323763	-0.046595	3.055265
238.598969	3074.855553	17.328768	-0.046567	3.051570
238.505160	3066.865892	17.333773	-0.046544	3.047873
238.549897	3058.858871	17.338778	-0.046547	3.044170
238.417325	3050.941182	17.343783	-0.046518	3.040495
238.204624	3042.952644	17.348787	-0.046473	3.036779
238.294111	3034.959439	17.353792	-0.046484	3.033071
238.217382	3026.932853	17.358797	-0.046465	3.029335
238.171584	3018.968612	17.363802	-0.046451	3.025625
238.117027	3011.014409	17.368807	-0.046436	3.021915
238.092219	3003.011410	17.373811	-0.046426	3.018178
238.016313	2995.049058	17.378816	-0.046407	3.014454
237.993022	2987.031719	17.383821	-0.046398	3.010701
238.153762	2979.025694	17.388826	-0.046422	3.006959
237.938014	2971.099129	17.393831	-0.046377	3.003230
237.843134	2963.101343	17.398835	-0.046354	2.999469
237.998295	2955.139632	17.403840	-0.046378	2.995733
238.015546	2947.110924	17.408845	-0.046376	2.991954
237.707421	2939.132821	17.413850	-0.046314	2.988178
237.602954	2931.142002	17.418855	-0.046289	2.984401
237.570753	2923.162904	17.423859	-0.046278	2.980628
237.684488	2915.195506	17.428864	-0.046294	2.976864
237.546715	2907.199149	17.433869	-0.046263	2.973068
237.423220	2899.202999	17.438874	-0.046235	2.969268
237.422034	2891.247386	17.443879	-0.046230	2.965489
237.138749	2883.283021	17.448883	-0.046172	2.961686
237.124069	2875.313231	17.453888	-0.046164	2.957890
237.174623	2867.313282	17.458893	-0.046168	2.954078
237.149016	2859.291347	17.463898	-0.046158	2.950246
237.225724	2851.304018	17.468903	-0.046168	2.946431
236.832952	2843.355717	17.473907	-0.046089	2.942606
236.993918	2835.374761	17.478912	-0.046114	2.938789
236.940299	2827.407279	17.483917	-0.046099	2.934962
236.991519	2819.381668	17.488922	-0.046103	2.931107
236.953633	2811.424937	17.493927	-0.046091	2.927276
236.625138	2803.465744	17.498931	-0.046025	2.923424
236.738570	2795.472690	17.503936	-0.046041	2.919573
236.731803	2787.524620	17.508941	-0.046035	2.915733
236.440948	2779.477667	17.513946	-0.045975	2.911824
236.480612	2771.467747	17.518951	-0.045978	2.907946
236.466943	2763.463442	17.523955	-0.045970	2.904063
236.427119	2755.536331	17.528960	-0.045957	2.900210
236.337007	2747.568251	17.533965	-0.045935	2.896330
236.267350	2739.572116	17.538970	-0.045917	2.892431
236.378616	2731.561582	17.543975	-0.045933	2.888531
236.110005	2723.618774	17.548979	-0.045878	2.884637
236.048394	2715.681624	17.553984	-0.045861	2.880753
236.047045	2707.682860	17.558989	-0.045856	2.876836
235.948005	2699.690647	17.563994	-0.045832	2.872911
236.127071	2691.673163	17.568999	-0.045861	2.868985
235.967338	2683.686186	17.574003	-0.045826	2.865049
236.037604	2675.750310	17.579008	-0.045834	2.861145
235.683664	2667.823013	17.584013	-0.045763	2.857217
235.794432	2659.805092	17.589018	-0.045778	2.853265
235.765093	2651.809006	17.594023	-0.045768	2.849310
235.497864	2643.830804	17.599027	-0.045713	2.845345
235.501880	2635.878416	17.604032	-0.045708	2.841402
235.466478	2627.915775	17.609037	-0.045697	2.837447
235.424263	2619.908556	17.614042	-0.045684	2.833464
235.530780	2611.885015	17.619047	-0.045698	2.829475
235.522225	2603.901510	17.624051	-0.045692	2.825494
235.232672	2595.968894	17.629056	-0.045633	2.821517
235.108526	2588.001841	17.634061	-0.045604	2.817527
235.155144	2580.010971	17.639066	-0.045608	2.813528
235.037314	2572.013004	17.644071	-0.045581	2.809511
234.931955	2564.052442	17.649075	-0.045556	2.805508
234.937437	2556.085552	17.654080	-0.045552	2.801502
234.944043	2548.119393	17.659085	-0.045548	2.797491
234.970646	2540.113468	17.664090	-0.045548	2.793455
234.841210	2532.115562	17.669095	-0.045519	2.789408
234.682934	2524.138850	17.674099	-0.045484	2.785365
234.567500	2516.212557	17.679104	-0.045458	2.781343
234.559103	2508.228738	17.684109	-0.045451	2.777293
234.588259	2500.219638	17.689114	-0.045451	2.773226
234.472480	2492.256990	17.694119	-0.045424	2.769169
234.241746	2484.285855	17.699123	-0.045376	2.765094
234.348807	2476.331624	17.704128	-0.045391	2.761042
234.251125	2468.355665	17.709133	-0.045368	2.756960
234.302983	2460.305091	17.714138	-0.045372	2.752844
234.148420	2452.307896	17.719143	-0.045338	2.748736
234.148352	2444.309976	17.724147	-0.045333	2.744631
234.141673	2436.381849	17.729152	-0.045327	2.740555
233.976894	2428.459395	17.734157	-0.045291	2.736466
234.140110	2420.419208	17.739162	-0.045316	2.732331
234.186700	2412.451474	17.744167	-0.045320	2.728219
233.897945	2404.507876	17.749171	-0.045261	2.724094
233.764828	2396.566357	17.754176	-0.045231	2.719972
233.874391	2388.585725	17.759181	-0.045247	2.715839
233.843204	2380.571556	17.764186	-0.045236	2.711674
233.800822	2372.611827	17.769191	-0.045223	2.707530
233.497211	2364.646553	17.774195	-0.045161	2.703360
233.561215	2356.688423	17.779200	-0.045168	2.699211
233.419795	2348.723646	17.784205	-0.045136	2.695038
233.349664	2340.728128	17.789210	-0.045118	2.690848
233.357848	2332.767774	17.794215	-0.045115	2.686675
233.315119	2324.772478	17.799219	-0.045101	2.682473
233.358207	2316.817293	17.804224	-0.045104	2.678291
233.170423	2308.858100	17.809229	-0.045064	2.674086
233.112270	2300.846119	17.814234	-0.045048	2.669855
233.073300	2292.884675	17.819239	-0.045036	2.665645
232.990364	2284.902289	17.824243	-0.045015	2.661415
233.029152	2276.940730	17.829248	-0.045018	2.657196
232.990374	2268.954274	17.834253	-0.045005	2.652953
232.927129	2260.967483	17.839258	-0.044988	2.648701
233.021257	2253.003234	17.844263	-0.045001	2.644464
232.862011	2245.064107	17.849267	-0.044966	2.640218
232.759381	2237.124747	17.854272	-0.044942	2.635968
232.923979	2229.093930	17.859277	-0.044967	2.631680
232.778880	2221.117527	17.864282	-0.044935	2.627393
232.618356	2213.184298	17.869287	-0.044900	2.623122
232.375258	2205.227913	17.874291	-0.044850	2.618826
232.389188	2197.249957	17.879296	-0.044847	2.614528
232.518046	2189.235865	17.884301	-0.044866	2.610211
232.245183	2181.302806	17.889306	-0.044810	2.605905
232.299799	2173.347407	17.894311	-0.044815	2.601600
232.257494	2165.373234	17.899315	-0.044802	2.597272
232.168896	2157.339500	17.904320	-0.044781	2.592902
232.144599	2149.235369	17.909325	-0.044771	2.588489
232.128086	2141.287423	17.914330	-0.044763	2.584155
232.050356	2133.397061	17.919335	-0.044743	2.579841
231.853215	2125.454259	17.924339	-0.044701	2.575483
232.016245	2117.459731	17.929344	-0.044727	2.571114
231.872174	2109.511454	17.934349	-0.044695	2.566742
231.851729	2101.549272	17.939354	-0.044686	2.562363
231.817360	2093.620878	17.944359	-0.044674	2.557994
231.506558	2085.666431	17.949363	-0.044611	2.553584
231.566866	2077.664141	17.954368	-0.044617	2.549166
231.695925	2069.682159	17.959373	-0.044636	2.544756
231.598231	2061.754883	17.964378	-0.044613	2.540353
231.466945	2053.821259	17.969383	-0.044583	2.535937
231.409318	2045.823744	17.974387	-0.044568	2.531482
231.436433	2037.851323	17.979392	-0.044567	2.527040
231.194889	2029.922272	17.984397	-0.044517	2.522594
231.092042	2021.962511	17.989402	-0.044493	2.518134
231.321102	2013.950072	17.994407	-0.044531	2.513660
231.017575	2005.975809	17.999411	-0.044469	2.509161
230.868885	1998.022148	18.004416	-0.044436	2.504677
231.097439	1990.034702	18.009421	-0.044474	2.500193
230.909796	1982.102778	18.014426	-0.044434	2.495702
230.813200	1974.153327	18.019431	-0.044411	2.491199
230.568906	1966.164212	18.024435	-0.044360	2.486656
230.648608	1958.212098	18.029440	-0.044370	2.482148
230.506637	1950.285079	18.034445	-0.044338	2.477630
230.347957	1942.311805	18.039450	-0.044303	2.473077
230.557245	1934.304794	18.044455	-0.044337	2.468523
230.589530	1926.307160	18.049459	-0.044338	2.463953
230.425509	1918.400098	18.054464	-0.044303	2.459411
230.320698	1910.447534	18.059469	-0.044278	2.454840
230.336865	1902.451663	18.064474	-0.044276	2.450244
230.303033	1894.511997	18.069479	-0.044264	2.445668
230.115704	1886.580097	18.074483	-0.044224	2.441076
230.247294	1878.608552	18.079488	-0.044244	2.436477
230.088791	1870.591966	18.084493	-0.044209	2.431821
229.973886	1862.596889	18.089498	-0.044183	2.427172
229.989929	1854.658874	18.094503	-0.044181	2.422557
230.014219	1846.700075	18.099507	-0.044180	2.417922
229.904025	1838.758594	18.104512	-0.044154	2.413278
229.604404	1830.813366	18.109517	-0.044093	2.408608
229.592976	1822.849912	18.114522	-0.044086	2.403940
229.739880	1814.896762	18.119527	-0.044108	2.399282
229.531534	1806.944062	18.124531	-0.044065	2.394587
229.461905	1798.969764	18.129536	-0.044047	2.389881
229.298393	1791.036973	18.134541	-0.044011	2.385183
229.292057	1783.070913	18.139546	-0.044005	2.380468
229.329008	1775.132439	18.144551	-0.044006	2.375764
229.269791	1767.139902	18.149555	-0.043990	2.371011
229.122069	1759.194194	18.154560	-0.043958	2.366269
229.036462	1751.256651	18.159565	-0.043937	2.361527
229.133822	1743.281964	18.164570	-0.043950	2.356768
229.163188	1735.317659	18.169575	-0.043950	2.352000
228.713919	1727.373202	18.174579	-0.043861	2.347196
228.788606	1719.409538	18.179584	-0.043870	2.342412
228.827442	1711.456338	18.184589	-0.043872	2.337623
228.463282	1703.529766	18.189594	-0.043799	2.332806
228.574458	1695.552512	18.194599	-0.043815	2.327988
228.553291	1687.587098	18.199603	-0.043806	2.323157
228.492973	1679.654638	18.204608	-0.043790	2.318332
228.245791	1671.727133	18.209613	-0.043738	2.313484
228.448636	1663.712112	18.214618	-0.043771	2.308610
228.557162	1655.758421	18.219623	-0.043786	2.303756
228.393774	1647.835071	18.224627	-0.043751	2.298887
228.072948	1639.915206	18.229632	-0.043686	2.293996
228.390368	1631.897458	18.234637	-0.043740	2.289089
228.206836	1623.973572	18.239642	-0.043700	2.284187
228.015958	1616.067572	18.244647	-0.043660	2.279284
228.079733	1608.099940	18.249651	-0.043667	2.274355
228.037200	1600.071297	18.254656	-0.043654	2.269368
227.826720	1592.129469	18.259661	-0.043609	2.264409
227.588449	1584.223533	18.264666	-0.043560	2.259459
227.761413	1576.265177	18.269671	-0.043587	2.254502
227.335419	1568.332621	18.274675	-0.043503	2.249497
227.431107	1560.364161	18.279680	-0.043515	2.244504
227.474205	1552.428623	18.284685	-0.043518	2.239517
227.325071	1544.497274	18.289690	-0.043485	2.234504
227.388780	1536.518732	18.294695	-0.043492	2.229468
227.448725	1528.530121	18.299699	-0.043498	2.224415
227.366168	1520.634146	18.304704	-0.043478	2.219396
227.378746	1512.683388	18.309709	-0.043475	2.214339
227.203771	1504.739748	18.314714	-0.043437	2.209258
227.450436	1496.772389	18.319719	-0.043478	2.204189
227.163929	1488.882591	18.324723	-0.043420	2.199109
226.885914	1480.969453	18.329728	-0.043363	2.194003
226.955708	1472.959072	18.334733	-0.043371	2.188855
226.753085	1465.025410	18.339738	-0.043328	2.183719
226.703782	1457.112178	18.344743	-0.043314	2.178598
226.746850	1449.132755	18.349747	-0.043316	2.173430
226.849235	1441.174622	18.354752	-0.043330	2.168269
226.661732	1433.262277	18.359757	-0.043290	2.163100
226.405618	1425.364423	18.364762	-0.043238	2.157920
226.612685	1417.393084	18.369767	-0.043271	2.152724
226.502773	1409.423413	18.374771	-0.043245	2.147486
226.391039	1401.510262	18.379776	-0.043220	2.142272
226.590883	1393.544074	18.384781	-0.043252	2.137041
226.537895	1385.598382	18.389786	-0.043237	2.131785
226.359084	1377.695340	18.394791	-0.043198	2.126534
226.298681	1369.757316	18.399795	-0.043182	2.121257
226.216925	1361.849409	18.404800	-0.043162	2.115985
226.118799	1353.850778	18.409805	-0.043138	2.110637
225.833025	1345.908921	18.414810	-0.043080	2.105296
225.975009	1337.984290	18.419815	-0.043101	2.099995
225.724114	1330.077376	18.424819	-0.043050	2.094653
225.619265	1322.128207	18.429824	-0.043025	2.089284
225.566944	1314.193740	18.434829	-0.043010	2.083916
225.505770	1306.273893	18.439834	-0.042994	2.078543
225.565010	1298.337268	18.444839	-0.043000	2.073156
225.501512	1290.377549	18.449843	-0.042983	2.067728
225.470492	1282.457751	18.454848	-0.042972	2.062316
225.544992	1274.532606	18.459853	-0.042981	2.056896
225.280608	1266.617062	18.464858	-0.042926	2.051435
225.377274	1258.668684	18.469863	-0.042939	2.045973
225.263897	1250.753313	18.474867	-0.042913	2.040498
225.045352	1242.869987	18.479872	-0.042867	2.035019
225.081002	1234.876712	18.484877	-0.042869	2.029476
225.037021	1226.940038	18.489882	-0.042855	2.023948
225.041122	1219.030689	18.494887	-0.042851	2.018429
224.829533	1211.121364	18.499891	-0.042807	2.012873
224.921994	1203.161684	18.504896	-0.042819	2.007297
224.926526	1195.249015	18.509901	-0.042815	2.001730
224.632091	1187.356525	18.514906	-0.042755	1.996131
224.563869	1179.436691	18.519911	-0.042737	1.990520
224.517663	1171.492005	18.524915	-0.042723	1.984878
224.270852	1163.615576	18.529920	-0.042672	1.979247
224.303557	1155.685306	18.534925	-0.042673	1.973591
224.294814	1147.733158	18.539930	-0.042666	1.967899
224.243813	1139.833335	18.544935	-0.042652	1.962223
224.007305	1131.940204	18.549939	-0.042603	1.956516
224.089613	1123.962228	18.554944	-0.042613	1.950765
224.179469	1116.013219	18.559949	-0.042625	1.945019
223.789982	1108.144414	18.564954	-0.042547	1.939262
223.862658	1100.223926	18.569959	-0.042555	1.933500
223.793793	1092.285776	18.574963	-0.042538	1.927693
223.776585	1084.379303	18.579968	-0.042529	1.921897
223.616032	1076.499235	18.584973	-0.042494	1.916088
223.454908	1068.580255	18.589978	-0.042459	1.910231
223.636218	1060.640114	18.594983	-0.042488	1.904380
223.431650	1052.760863	18.599987	-0.042445	1.898512
223.552995	1044.827295	18.604992	-0.042462	1.892622
223.514936	1036.912454	18.609997	-0.042450	1.886710
223.308018	1029.030640	18.615002	-0.042406	1.880785
223.318148	1021.143004	18.620007	-0.042403	1.874861
223.103077	1013.217826	18.625011	-0.042358	1.868865
223.265047	1005.271956	18.630016	-0.042383	1.862877
223.008639	997.420605	18.635021	-0.042330	1.856893
222.997421	989.486931	18.640026	-0.042323	1.850855
223.029723	981.581832	18.645031	-0.042324	1.844825
222.886396	973.705269	18.650035	-0.042292	1.838776
222.887259	965.808202	18.655040	-0.042288	1.832708
222.744724	957.903936	18.660045	-0.042256	1.826597
222.362211	950.048490	18.665050	-0.042180	1.820475
222.411192	942.149963	18.670055	-0.042184	1.814351
222.421166	934.216811	18.675059	-0.042181	1.808174
222.296420	926.349904	18.680064	-0.042152	1.802012
222.287037	918.456931	18.685069	-0.042145	1.795821
222.055809	910.522366	18.690074	-0.042097	1.789550
222.185282	902.605749	18.695079	-0.042116	1.783315
221.898139	894.751932	18.700083	-0.042058	1.777056
221.877165	886.843416	18.705088	-0.042049	1.770765
222.129998	878.914053	18.710093	-0.042091	1.764469
221.881281	871.084556	18.715098	-0.042039	1.758167
221.765852	863.213054	18.720103	-0.042013	1.751826
221.848378	855.288539	18.725107	-0.042023	1.745444
221.655097	847.448008	18.730112	-0.041982	1.739071
221.575809	839.568428	18.735117	-0.041962	1.732658
221.605130	831.654384	18.740122	-0.041963	1.726207
221.658605	823.785458	18.745127	-0.041968	1.719771
221.390456	815.950238	18.750131	-0.041913	1.713298
221.193220	808.064159	18.755136	-0.041871	1.706767
221.233989	800.168970	18.760141	-0.041873	1.700235
221.004025	792.325988	18.765146	-0.041826	1.693685
220.961985	784.440856	18.770151	-0.041813	1.687099
220.758232	776.586811	18.775155	-0.041770	1.680492
220.879789	768.708892	18.780160	-0.041787	1.673882
220.738478	760.840349	18.785165	-0.041756	1.667219
220.711303	752.955806	18.790170	-0.041746	1.660531
220.787862	745.097289	18.795175	-0.041755	1.653852
220.722037	737.218691	18.800179	-0.041738	1.647109
220.362133	729.415808	18.805184	-0.041666	1.640363
220.257029	721.561984	18.810189	-0.041641	1.633581
220.089877	713.651195	18.815194	-0.041605	1.626712
220.027296	705.800029	18.820199	-0.041588	1.619880
219.872020	697.961849	18.825203	-0.041554	1.613018
219.945589	690.078107	18.830208	-0.041563	1.606119
219.907763	682.246512	18.835213	-0.041551	1.599220
219.522094	674.443300	18.840218	-0.041474	1.592267
219.750951	666.533829	18.845223	-0.041512	1.585277
219.564714	658.723906	18.850227	-0.041472	1.578284
219.396337	650.890027	18.855232	-0.041435	1.571242
219.412497	643.034732	18.860237	-0.041433	1.564176
219.575000	635.179793	18.865242	-0.041459	1.557099
219.413875	627.354569	18.870247	-0.041424	1.549970
219.299823	619.512406	18.875251	-0.041397	1.542799
219.293686	611.683964	18.880256	-0.041391	1.535623
219.151472	603.863582	18.885261	-0.041360	1.528400
219.111453	596.026079	18.890266	-0.041347	1.521143
219.127808	588.219937	18.895271	-0.041345	1.513888
218.667720	580.436280	18.900275	-0.041255	1.506547
218.719152	572.600857	18.905280	-0.041259	1.499200
218.638706	564.794047	18.910285	-0.041239	1.491823
218.493363	556.977178	18.915290	-0.041207	1.484390
218.460076	549.184774	18.920295	-0.041196	1.476960
218.280367	541.332455	18.925299	-0.041157	1.469412
218.298599	533.502810	18.930304	-0.041156	1.461879
218.211733	525.718931	18.935309	-0.041135	1.454333
218.052347	517.913426	18.940314	-0.041100	1.446716
218.069131	510.126936	18.945319	-0.041098	1.439106
217.923454	502.341784	18.950323	-0.041066	1.431430
217.916575	494.541826	18.955328	-0.041060	1.423720
217.851246	486.768762	18.960333	-0.041042	1.415986
217.654867	478.985973	18.965338	-0.041001	1.408178
217.639390	471.209840	18.970343	-0.040993	1.400363
217.592766	463.429488	18.975347	-0.040979	1.392494
217.309708	455.669506	18.980352	-0.040922	1.384562
217.265196	447.899494	18.985357	-0.040908	1.376614
217.071119	440.132552	18.990362	-0.040867	1.368597
216.987730	432.380903	18.995367	-0.040847	1.360569
216.909479	424.631929	19.000371	-0.040827	1.352496
216.703648	416.877612	19.005376	-0.040784	1.344346
216.626724	409.138696	19.010381	-0.040765	1.336186
216.526681	401.376834	19.015386	-0.040741	1.327947
216.517041	393.636151	19.020391	-0.040734	1.319696
216.362400	385.841043	19.025395	-0.040700	1.311308
216.261134	378.043229	19.030400	-0.040677	1.302872
216.238031	370.323999	19.035405	-0.040667	1.294482
216.032770	362.612641	19.040410	-0.040624	1.286012
216.148859	354.893397	19.045415	-0.040641	1.277536
215.843515	347.213440	19.050419	-0.040579	1.268969
215.519973	339.545823	19.055424	-0.040514	1.260354
215.414935	331.849057	19.060429	-0.040489	1.251688
215.308689	324.141619	19.065434	-0.040465	1.242949
215.134363	316.480570	19.070439	-0.040427	1.234188
214.834597	308.793531	19.075443	-0.040367	1.225310
214.788464	301.104798	19.080448	-0.040353	1.216415
214.577282	293.438445	19.085453	-0.040309	1.207448
214.146410	285.825394	19.090458	-0.040224	1.198432
213.971836	278.175195	19.095463	-0.040186	1.189356
213.739133	270.523582	19.100467	-0.040138	1.180196
213.560524	262.880899	19.105472	-0.040100	1.170986
213.306277	255.261661	19.110477	-0.040048	1.161716
212.932026	247.646835	19.115482	-0.039973	1.152352
212.605079	240.016091	19.120487	-0.039907	1.142900
212.394415	232.392725	19.125491	-0.039863	1.133404
212.139722	224.792360	19.130496	-0.039811	1.123847
211.743319	217.234035	19.135501	-0.039732	1.114231
211.442442	209.639984	19.140506	-0.039671	1.104505
211.233712	202.066508	19.145511	-0.039628	1.094741
210.833897	194.513708	19.150515	-0.039548	1.084872
210.268327	187.012911	19.155520	-0.039438	1.074943
209.815934	179.474635	19.160525	-0.039349	1.064897
209.275475	171.962546	19.165530	-0.039244	1.054771
208.866918	164.444684	19.170535	-0.039163	1.044568
208.672128	156.908020	19.175539	-0.039122	1.034290
208.310876	149.400424	19.180544	-0.039050	1.023909
207.942014	141.922563	19.185549	-0.038976	1.013461
207.320209	134.481535	19.190554	-0.038856	1.002894
207.024210	126.998399	19.195559	-0.038796	0.992235
206.306184	119.571070	19.200563	-0.038657	0.981434
205.775239	112.154958	19.205568	-0.038554	0.970576
205.455289	104.718650	19.210573	-0.038489	0.959620
204.879231	97.332390	19.215578	-0.038377	0.948545
204.666068	89.913768	19.220583	-0.038333	0.937386
204.208701	82.539017	19.225587	-0.038243	0.926093
203.680563	75.208212	19.230592	-0.038140	0.914710
202.972755	67.903997	19.235597	-0.038003	0.903175
202.396894	60.828337	19.240602	-0.037892	0.891889