Thu Mar 11 20:32:49 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.675266	-0.119342	0.000000	-0.000043	0.722388

0.627575	-0.117936	0.005005	-0.000034	0.722374
0.529745	-0.099969	0.010010	-0.000016	0.722375
0.833382	-0.153447	0.015014	-0.000073	0.722377
0.582177	-0.113935	0.020019	-0.000026	0.722367
0.932223	-0.168800	0.025024	-0.000091	0.722381
0.577032	-0.110414	0.030029	-0.000025	0.722372
0.801925	-0.148480	0.035034	-0.000067	0.722376
0.742377	-0.136853	0.040038	-0.000056	0.722378
0.661529	-0.125409	0.045043	-0.000041	0.722373
0.661448	-0.119520	0.050048	-0.000041	0.722384
0.673530	-0.126253	0.055053	-0.000044	0.722376
0.852823	-0.157074	0.060058	-0.000077	0.722378
0.918673	-0.201721	0.065062	-0.000089	0.722313
0.759238	-0.293400	0.070067	-0.000060	0.722078
0.730027	-0.282923	0.075072	-0.000054	0.722088
0.574264	-0.259886	0.080077	-0.000025	0.722079
0.688927	-0.279876	0.085082	-0.000047	0.722080
0.726138	-0.284922	0.090086	-0.000054	0.722084
0.542504	-0.256564	0.095091	-0.000020	0.722075
0.499870	-0.359189	0.100096	-0.000012	0.721859
0.583903	-0.429650	0.105101	-0.000028	0.721750
0.670835	-0.445735	0.110106	-0.000044	0.721749
0.631203	-0.436979	0.115110	-0.000037	0.721752
0.653792	-0.441964	0.120115	-0.000041	0.721751
0.985175	-0.596926	0.125120	-0.000103	0.721562
0.759799	-0.616874	0.130125	-0.000061	0.721444
0.603201	-0.589038	0.135130	-0.000032	0.721444
0.737464	-0.612003	0.140134	-0.000057	0.721446
0.828382	-0.716484	0.145139	-0.000074	0.721273
0.760288	-0.776638	0.150144	-0.000061	0.721131
0.816446	-0.788036	0.155149	-0.000072	0.721129
0.802941	-0.784808	0.160154	-0.000069	0.721130
0.525754	-0.852145	0.165158	-0.000018	0.720901
0.537248	-0.866459	0.170163	-0.000020	0.720877
0.855903	-0.917938	0.175168	-0.000079	0.720887
0.730217	-0.992544	0.180173	-0.000056	0.720697
0.607921	-1.048895	0.185178	-0.000033	0.720543
0.474762	-1.022297	0.190182	-0.000008	0.720549
0.459134	-1.088231	0.195187	-0.000006	0.720414
0.513439	-1.189674	0.200192	-0.000016	0.720233
0.447552	-1.182151	0.205197	-0.000004	0.720225
0.511181	-1.265101	0.210202	-0.000015	0.720084
0.755400	-1.398977	0.215206	-0.000061	0.719907
0.605355	-1.375830	0.220211	-0.000033	0.719900
0.530461	-1.469169	0.225216	-0.000019	0.719690
0.593064	-1.522780	0.230221	-0.000031	0.719606
0.693659	-1.571868	0.235226	-0.000050	0.719545
0.567619	-1.684940	0.240230	-0.000026	0.719278
0.285523	-1.639895	0.245235	0.000026	0.719268
0.197154	-1.724210	0.250240	0.000043	0.719071
0.371372	-1.811313	0.255245	0.000010	0.718960
0.425526	-1.859223	0.260250	-0.000000	0.718885
0.208277	-1.939711	0.265254	0.000040	0.718650
0.132183	-1.931507	0.270259	0.000054	0.718639
0.089724	-2.047590	0.275264	0.000062	0.718396
0.019447	-2.053900	0.280269	0.000075	0.718359
-0.089254	-2.130830	0.285274	0.000095	0.718169
0.104211	-2.237295	0.290278	0.000059	0.718027
0.141641	-2.304024	0.295283	0.000052	0.717908
0.048096	-2.385765	0.300288	0.000070	0.717714
-0.271357	-2.361772	0.305293	0.000129	0.717649
-0.616689	-2.434829	0.310298	0.000193	0.717383
-2.330826	-2.127544	0.315302	0.000512	0.717387
-1.894801	-2.309771	0.320307	0.000431	0.717181
-3.079617	-2.143762	0.325312	0.000652	0.717092
-2.923518	-2.173984	0.330317	0.000622	0.717087
-2.916918	-2.285473	0.335322	0.000621	0.716869
-4.354559	-2.083475	0.340326	0.000889	0.716762
-4.379978	-2.084242	0.345331	0.000893	0.716752
-3.773514	-2.193778	0.350336	0.000780	0.716749
-4.786746	-2.164037	0.355341	0.000969	0.716451
-5.056663	-2.116322	0.360346	0.001019	0.716450
-4.796270	-2.160035	0.365350	0.000970	0.716456
-5.181117	-2.096104	0.370355	0.001042	0.716447
-5.607737	-2.172481	0.375360	0.001121	0.716145
-6.138497	-2.083776	0.380365	0.001220	0.716134
-5.978059	-2.112405	0.385370	0.001190	0.716134
-5.705075	-2.158995	0.390374	0.001139	0.716138
-6.185822	-2.117888	0.395379	0.001229	0.716050
-6.749338	-2.097204	0.400384	0.001333	0.715892
-6.589971	-2.129188	0.405389	0.001304	0.715885
-7.150734	-2.028635	0.410394	0.001408	0.715887
-6.712659	-2.104635	0.415398	0.001326	0.715891
-6.586120	-2.202961	0.420403	0.001303	0.715741
-7.893440	-2.064894	0.425408	0.001546	0.715553
-7.692973	-2.102072	0.430413	0.001509	0.715551
-7.518223	-2.133883	0.435418	0.001476	0.715549
-7.602715	-2.115889	0.440422	0.001492	0.715555
-7.992802	-2.059123	0.445427	0.001564	0.715530
-8.340295	-2.146278	0.450432	0.001629	0.715235
-8.420877	-2.134884	0.455437	0.001644	0.715229
-9.072069	-2.017785	0.460442	0.001765	0.715232
-8.617606	-2.095254	0.465446	0.001680	0.715239
-8.798984	-2.067556	0.470451	0.001714	0.715230
-8.484592	-2.138920	0.475456	0.001655	0.715199
-9.566172	-2.092157	0.480461	0.001856	0.714910
-9.626293	-2.081929	0.485466	0.001868	0.714909
-9.480199	-2.105567	0.490470	0.001840	0.714914
-9.663461	-2.079418	0.495475	0.001874	0.714901
-9.668426	-2.071543	0.500480	0.001875	0.714915
-9.533364	-2.099115	0.505485	0.001850	0.714909
-9.982366	-2.127356	0.510490	0.001933	0.714694
-10.556482	-2.066406	0.515494	0.002040	0.714612
-10.531772	-2.075615	0.520499	0.002035	0.714603
-10.178864	-2.133505	0.525504	0.001970	0.714613
-10.603761	-2.061081	0.530509	0.002049	0.714607
-10.561220	-2.067766	0.535514	0.002041	0.714609
-10.221489	-2.155505	0.540518	0.001977	0.714555
-11.644007	-2.042746	0.545523	0.002242	0.714275
-11.402519	-2.082086	0.550528	0.002197	0.714283
-11.054941	-2.148500	0.555533	0.002132	0.714274
-11.477467	-2.072605	0.560538	0.002211	0.714276
-11.236044	-2.113033	0.565542	0.002166	0.714281
-11.432872	-2.081828	0.570547	0.002202	0.714273
-11.284681	-2.181634	0.575552	0.002175	0.714128
-12.481892	-2.048402	0.580557	0.002397	0.713969
-12.405156	-2.061298	0.585562	0.002383	0.713971
-12.022563	-2.126409	0.590566	0.002312	0.713977
-12.631046	-2.021899	0.595571	0.002425	0.713969
-12.446167	-2.050841	0.600576	0.002390	0.713977
-11.984010	-2.135194	0.605581	0.002304	0.713974
-12.522000	-2.119509	0.610586	0.002404	0.713814
-13.469959	-2.027973	0.615590	0.002581	0.713661
-13.069206	-2.105313	0.620595	0.002506	0.713649
-13.075310	-2.099289	0.625600	0.002507	0.713659
-13.523177	-2.023234	0.630605	0.002590	0.713652
-13.278543	-2.066085	0.635610	0.002545	0.713654
-12.875869	-2.135561	0.640614	0.002470	0.713658
-13.420124	-2.089164	0.645619	0.002571	0.713558
-14.185844	-2.049805	0.650624	0.002713	0.713365
-13.662773	-2.146268	0.655629	0.002616	0.713359
-14.366993	-2.019984	0.660634	0.002747	0.713361
-14.313689	-2.026313	0.665638	0.002737	0.713367
-14.062550	-2.075032	0.670643	0.002690	0.713359
-14.011484	-2.079864	0.675648	0.002681	0.713368
-14.019186	-2.127315	0.680653	0.002682	0.713271
-14.948115	-2.086368	0.685658	0.002855	0.713023
-14.606195	-2.143495	0.690662	0.002791	0.713031
-15.284318	-2.028330	0.695667	0.002917	0.713020
-15.388442	-2.004022	0.700672	0.002936	0.713032
-15.008087	-2.074234	0.705677	0.002866	0.713027
-15.160803	-2.046094	0.710682	0.002894	0.713029
-15.122603	-2.053891	0.715686	0.002887	0.713027
-15.713403	-2.108192	0.720691	0.002997	0.712710
-16.025189	-2.048219	0.725696	0.003055	0.712719
-16.322395	-1.998567	0.730701	0.003110	0.712712
-16.292117	-2.005266	0.735706	0.003104	0.712710
-15.797317	-2.090813	0.740710	0.003012	0.712715
-16.114172	-2.038993	0.745715	0.003071	0.712706
-16.016527	-2.052050	0.750720	0.003052	0.712715
-15.740686	-2.178433	0.755725	0.003001	0.712561
-17.068662	-2.029648	0.760730	0.003248	0.712387
-16.686732	-2.095008	0.765734	0.003177	0.712392
-17.114039	-2.022956	0.770739	0.003256	0.712384
-16.847756	-2.067239	0.775744	0.003207	0.712391
-16.686110	-2.098600	0.780749	0.003177	0.712386
-17.111951	-2.024026	0.785754	0.003256	0.712383
-16.688926	-2.157793	0.790758	0.003177	0.712267
-17.976632	-2.020136	0.795763	0.003417	0.712085
-17.650630	-2.074044	0.800768	0.003356	0.712093
-17.550865	-2.092654	0.805773	0.003337	0.712092
-17.651292	-2.076846	0.810778	0.003356	0.712088
-17.698375	-2.065765	0.815782	0.003364	0.712093
-18.149881	-1.989279	0.820787	0.003448	0.712085
-17.591684	-2.145972	0.825792	0.003344	0.711972
-18.685899	-2.058878	0.830797	0.003548	0.711757
-18.949146	-2.012646	0.835802	0.003597	0.711755
-18.651918	-2.063193	0.840806	0.003541	0.711760
-18.541815	-2.087560	0.845811	0.003521	0.711751
-18.803784	-2.035918	0.850816	0.003570	0.711761
-18.830230	-2.033174	0.855821	0.003574	0.711758
-18.756589	-2.046229	0.860826	0.003561	0.711758
-19.098506	-2.126258	0.865830	0.003624	0.711477
-19.680450	-2.036892	0.870835	0.003732	0.711449
-19.442155	-2.076313	0.875840	0.003688	0.711455
-19.074475	-2.142312	0.880845	0.003619	0.711454
-19.749261	-2.021415	0.885850	0.003745	0.711455
-19.391585	-2.082774	0.890854	0.003678	0.711460
-19.416878	-2.104574	0.895859	0.003683	0.711408
-20.456752	-2.054445	0.900864	0.003876	0.711139
-20.541332	-2.040401	0.905869	0.003892	0.711137
-20.536849	-2.041797	0.910874	0.003891	0.711136
-20.256448	-2.089350	0.915878	0.003839	0.711141
-20.653157	-2.021445	0.920883	0.003913	0.711135
-20.643686	-2.018333	0.925888	0.003911	0.711145
-20.354065	-2.072769	0.930893	0.003857	0.711140
-21.114531	-2.038397	0.935898	0.003998	0.710938
-21.433115	-2.014010	0.940902	0.004057	0.710873
-21.212512	-2.057711	0.945907	0.004016	0.710865
-21.304422	-2.036730	0.950912	0.004033	0.710874
-21.490015	-2.004411	0.955917	0.004068	0.710873
-21.080524	-2.080991	0.960922	0.003991	0.710866
-20.877294	-2.111470	0.965926	0.003954	0.710877
-21.754731	-2.091700	0.970931	0.004117	0.710605
-22.288277	-2.030396	0.975936	0.004216	0.710538
-22.050060	-2.073679	0.980941	0.004172	0.710536
-22.321054	-2.027898	0.985946	0.004222	0.710531
-22.240802	-2.038537	0.990950	0.004207	0.710539
-21.970097	-2.091947	0.995955	0.004156	0.710529
-22.114994	-2.063128	1.000960	0.004183	0.710535
-22.344479	-2.144145	1.005965	0.004226	0.710291
-23.084548	-2.048597	1.010970	0.004364	0.710219
-22.984271	-2.064838	1.015974	0.004345	0.710223
-23.245544	-2.022350	1.020979	0.004393	0.710215
-23.059573	-2.051635	1.025984	0.004359	0.710222
-22.785937	-2.103965	1.030989	0.004308	0.710215
-23.253632	-2.020394	1.035994	0.004395	0.710216
-23.465695	-2.109807	1.040998	0.004434	0.709962
-24.105195	-2.032004	1.046003	0.004553	0.709890
-23.908273	-2.063205	1.051008	0.004516	0.709898
-23.830591	-2.078154	1.056013	0.004502	0.709896
-24.263844	-2.002476	1.061018	0.004582	0.709893
-23.670581	-2.105598	1.066022	0.004472	0.709898
-24.004160	-2.052056	1.071027	0.004534	0.709887
-24.270050	-2.111754	1.076032	0.004583	0.709673
-24.705581	-2.072938	1.081037	0.004664	0.709595
-24.970828	-2.027941	1.086042	0.004713	0.709591
-24.765073	-2.060289	1.091046	0.004675	0.709600
-24.723597	-2.073116	1.096051	0.004667	0.709589
-24.641799	-2.083334	1.101056	0.004652	0.709598
-24.692405	-2.075965	1.106061	0.004661	0.709595
-25.423683	-2.096209	1.111066	0.004797	0.709294
-25.612237	-2.073733	1.116070	0.004832	0.709272
-26.050437	-2.001342	1.121075	0.004914	0.709261
-25.779317	-2.047839	1.126080	0.004863	0.709264
-25.505001	-2.096895	1.131085	0.004812	0.709264
-25.914529	-2.025714	1.136090	0.004888	0.709261
-25.898402	-2.023918	1.141094	0.004885	0.709270
-25.898873	-2.103368	1.146099	0.004885	0.709111
-26.851574	-2.008760	1.151104	0.005062	0.708961
-26.545054	-2.063440	1.156109	0.005005	0.708961
-26.757597	-2.029781	1.161114	0.005045	0.708953
-26.305515	-2.106271	1.166118	0.004961	0.708961
-26.694400	-2.040287	1.171123	0.005033	0.708955
-26.917772	-1.997135	1.176128	0.005074	0.708962
-26.521802	-2.126584	1.181133	0.005001	0.708844
-27.810011	-2.000517	1.186138	0.005240	0.708637
-27.295680	-2.087598	1.191142	0.005144	0.708646
-27.474590	-2.060594	1.196147	0.005178	0.708636
-27.434282	-2.064476	1.201152	0.005170	0.708643
-27.632831	-2.030153	1.206157	0.005207	0.708641
-27.978801	-1.970216	1.211162	0.005271	0.708638
-27.410801	-2.096440	1.216166	0.005165	0.708588
-28.318333	-2.055162	1.221171	0.005334	0.708347
-28.480662	-2.023709	1.226176	0.005364	0.708352
-28.491875	-2.022500	1.231181	0.005366	0.708351
-28.431323	-2.035329	1.236186	0.005355	0.708347
-28.532839	-2.014248	1.241190	0.005374	0.708353
-28.610039	-2.004628	1.246195	0.005388	0.708345
-28.388311	-2.040302	1.251200	0.005347	0.708353
-28.702462	-2.139005	1.256205	0.005405	0.708043
-29.690374	-1.980648	1.261210	0.005589	0.708008
-28.971916	-2.102291	1.266214	0.005455	0.708021
-29.087556	-2.086908	1.271219	0.005477	0.708010
-29.409752	-2.026884	1.276224	0.005536	0.708016
-29.143874	-2.075452	1.281229	0.005487	0.708014
-29.303924	-2.067103	1.286234	0.005517	0.707973
-30.189912	-2.042546	1.291238	0.005681	0.707706
-30.370383	-2.014982	1.296243	0.005715	0.707697
-30.183581	-2.045954	1.301248	0.005680	0.707702
-30.155039	-2.050702	1.306253	0.005675	0.707703
-30.476571	-1.996244	1.311258	0.005734	0.707697
-30.198223	-2.041899	1.316262	0.005683	0.707705
-30.225163	-2.041973	1.321267	0.005687	0.707696
-30.327019	-2.140592	1.326272	0.005706	0.707462
-31.436334	-1.984379	1.331277	0.005913	0.707378
-31.392902	-1.994582	1.336282	0.005905	0.707374
-31.180056	-2.028253	1.341286	0.005865	0.707382
-31.287204	-2.013873	1.346291	0.005885	0.707373
-30.842774	-2.089795	1.351296	0.005802	0.707380
-30.985743	-2.066384	1.356301	0.005828	0.707376
-31.433030	-2.062546	1.361306	0.005912	0.707224
-32.025481	-2.024961	1.366310	0.006022	0.707087
-31.853890	-2.059758	1.371315	0.005990	0.707079
-32.216853	-1.990678	1.376320	0.006057	0.707088
-32.115267	-2.010391	1.381325	0.006038	0.707085
-31.792045	-2.069960	1.386330	0.005978	0.707081
-31.885919	-2.051294	1.391334	0.005995	0.707085
-32.101975	-2.095247	1.396339	0.006036	0.706920
-32.936682	-2.028087	1.401344	0.006191	0.706756
-32.655965	-2.078759	1.406349	0.006139	0.706755
-33.152464	-1.990851	1.411354	0.006231	0.706754
-32.729184	-2.062582	1.416358	0.006152	0.706762
-32.754296	-2.062975	1.421363	0.006157	0.706752
-33.216922	-1.977452	1.426368	0.006243	0.706759
-33.051106	-2.062275	1.431373	0.006212	0.706648
-34.059567	-1.985704	1.436378	0.006399	0.706441
-33.767158	-2.032789	1.441382	0.006345	0.706451
-34.087189	-1.979365	1.446387	0.006404	0.706444
-33.955596	-2.001242	1.451392	0.006380	0.706447
-33.533821	-2.076981	1.456397	0.006301	0.706446
-33.850985	-2.023330	1.461402	0.006360	0.706441
-33.773839	-2.044939	1.466406	0.006346	0.706425
-34.500861	-2.065363	1.471411	0.006481	0.706124
-34.764035	-2.014967	1.476416	0.006530	0.706131
-34.613171	-2.043735	1.481421	0.006502	0.706127
-34.671019	-2.035414	1.486426	0.006512	0.706123
-34.555197	-2.051608	1.491430	0.006491	0.706133
-35.145747	-1.949997	1.496435	0.006600	0.706125
-34.962902	-1.980700	1.501440	0.006566	0.706129
-34.736787	-2.122568	1.506445	0.006524	0.705925
-35.629327	-1.995336	1.511450	0.006690	0.705861
-35.345094	-2.042911	1.516454	0.006637	0.705868
-35.268090	-2.060414	1.521459	0.006623	0.705860
-35.774350	-1.966607	1.526464	0.006717	0.705868
-35.616427	-1.995857	1.531469	0.006687	0.705866
-35.653482	-1.991630	1.536474	0.006694	0.705861
-35.924935	-2.105510	1.541478	0.006745	0.705535
-36.369396	-2.033270	1.546483	0.006827	0.705521
-36.408520	-2.023553	1.551488	0.006835	0.705527
-36.104480	-2.076990	1.556493	0.006778	0.705528
-36.859386	-1.946266	1.561498	0.006918	0.705521
-36.470303	-2.011022	1.566502	0.006846	0.705530
-36.079943	-2.106456	1.571507	0.006773	0.705478
-37.260339	-2.025522	1.576512	0.006993	0.705218
-37.372725	-2.006700	1.581517	0.007013	0.705216
-37.506595	-1.986724	1.586522	0.007038	0.705208
-36.956468	-2.080504	1.591526	0.006936	0.705217
-37.369578	-2.011251	1.596531	0.007013	0.705208
-37.560652	-1.973477	1.601536	0.007048	0.705216
-37.107397	-2.070885	1.606541	0.006964	0.705183
-38.099243	-2.040439	1.611546	0.007148	0.704888
-37.997224	-2.054918	1.616550	0.007129	0.704896
-38.184053	-2.025652	1.621555	0.007164	0.704888
-38.093299	-2.039324	1.626560	0.007147	0.704893
-38.086735	-2.041359	1.631565	0.007146	0.704891
-38.170038	-2.029813	1.636570	0.007161	0.704885
-37.840453	-2.134423	1.641574	0.007100	0.704793
-39.126310	-2.007627	1.646579	0.007339	0.704587
-38.885275	-2.047511	1.651584	0.007294	0.704593
-38.603843	-2.097580	1.656589	0.007241	0.704593
-38.966004	-2.034963	1.661594	0.007309	0.704590
-38.924984	-2.037601	1.666598	0.007301	0.704599
-38.856097	-2.054580	1.671603	0.007288	0.704590
-39.176376	-2.103263	1.676608	0.007348	0.704377
-40.272156	-1.962085	1.681613	0.007551	0.704268
-39.987242	-2.015215	1.686618	0.007498	0.704263
-39.466629	-2.103669	1.691622	0.007401	0.704272
-40.052044	-2.003144	1.696627	0.007510	0.704265
-40.129272	-1.986406	1.701632	0.007525	0.704271
-39.566189	-2.089361	1.706637	0.007420	0.704266
-39.919879	-2.114579	1.711642	0.007485	0.704088
-40.872672	-2.006839	1.716646	0.007663	0.703963
-40.688860	-2.044227	1.721651	0.007628	0.703954
-40.709041	-2.037854	1.726656	0.007632	0.703960
-40.844865	-2.013263	1.731661	0.007657	0.703961
-40.665687	-2.048045	1.736666	0.007624	0.703955
-40.568794	-2.061152	1.741670	0.007606	0.703964
-41.211652	-2.046844	1.746675	0.007725	0.703761
-42.163123	-1.936830	1.751680	0.007902	0.703641
-41.455181	-2.062094	1.756685	0.007770	0.703643
-41.742385	-2.013762	1.761690	0.007824	0.703638
-41.989959	-1.966462	1.766694	0.007870	0.703644
-41.607241	-2.037262	1.771699	0.007798	0.703639
-41.453252	-2.063413	1.776704	0.007770	0.703642
-41.789560	-2.035916	1.781709	0.007832	0.703577
-42.735906	-1.983211	1.786714	0.008008	0.703343
-42.196110	-2.074130	1.791718	0.007908	0.703354
-42.822909	-1.968883	1.796723	0.008024	0.703341
-42.477831	-2.027366	1.801728	0.007960	0.703347
-41.960488	-2.119153	1.806733	0.007864	0.703348
-42.456707	-2.033707	1.811738	0.007956	0.703342
-42.610627	-2.090050	1.816742	0.007984	0.703173
-43.546244	-2.007575	1.821747	0.008159	0.703003
-43.244193	-2.058853	1.826752	0.008102	0.703009
-43.246397	-2.055690	1.831757	0.008103	0.703014
-43.685931	-1.979884	1.836762	0.008184	0.703009
-43.156373	-2.070644	1.841766	0.008086	0.703017
-43.357217	-2.040178	1.846771	0.008123	0.703006
-43.566883	-2.084375	1.851776	0.008162	0.702842
-44.146448	-2.052671	1.856781	0.008270	0.702697
-43.895784	-2.101163	1.861786	0.008223	0.702690
-44.039648	-2.070386	1.866790	0.008250	0.702700
-44.314717	-2.025176	1.871795	0.008301	0.702693
-44.001602	-2.080631	1.876800	0.008242	0.702694
-44.347659	-2.017549	1.881805	0.008307	0.702697
-45.015429	-2.035706	1.886810	0.008431	0.702419
-44.956334	-2.066486	1.891814	0.008420	0.702379
-45.112385	-2.043654	1.896819	0.008449	0.702369
-45.225795	-2.019545	1.901824	0.008470	0.702377
-44.831620	-2.089763	1.906829	0.008396	0.702377
-45.057664	-2.053331	1.911834	0.008438	0.702369
-45.153367	-2.033344	1.916838	0.008456	0.702376
-45.426945	-2.101653	1.921843	0.008507	0.702139
-46.083068	-2.015430	1.926848	0.008629	0.702077
-46.005705	-2.028156	1.931853	0.008614	0.702079
-46.154138	-2.002395	1.936858	0.008642	0.702078
-45.945548	-2.037324	1.941862	0.008603	0.702083
-45.874182	-2.056275	1.946867	0.008590	0.702070
-46.426291	-1.957029	1.951872	0.008692	0.702072
-46.065867	-2.111868	1.956877	0.008625	0.701889
-47.062301	-2.005877	1.961882	0.008811	0.701744
-46.683940	-2.069422	1.966886	0.008740	0.701752
-46.929130	-2.029763	1.971891	0.008786	0.701744
-46.912982	-2.031343	1.976896	0.008783	0.701747
-46.566304	-2.092517	1.981901	0.008718	0.701749
-47.071466	-2.004264	1.986906	0.008812	0.701745
-47.121926	-2.099599	1.991910	0.008821	0.701534
-47.810694	-2.024370	1.996915	0.008949	0.701438
-47.953212	-1.995337	2.001920	0.008976	0.701445

-47.682544	-2.045826	2.011917	0.008925	0.701441
-47.817023	-2.022333	2.021914	0.008950	0.701441
-47.777991	-2.030050	2.031910	0.008943	0.701440
-47.929684	-2.003835	2.041907	0.008971	0.701438
-47.871163	-2.013020	2.051904	0.008960	0.701441
-48.028352	-2.046889	2.061901	0.008989	0.701316
-48.048688	-1.983573	2.071898	0.008992	0.701437
-47.585271	-2.066001	2.081894	0.008906	0.701438
-47.436893	-2.091788	2.091891	0.008878	0.701440
-47.866612	-2.014837	2.101888	0.008958	0.701441
-47.524832	-2.078624	2.111885	0.008894	0.701435
-47.764034	-2.035724	2.121882	0.008938	0.701436
-47.614872	-2.062732	2.131878	0.008910	0.701436
-47.529765	-2.078395	2.141875	0.008894	0.701435
-47.251520	-2.014212	2.151872	0.008842	0.701666
-46.791288	-2.058648	2.161869	0.008756	0.701742
-47.112176	-2.001105	2.171866	0.008816	0.701743
-46.794741	-2.057384	2.181862	0.008757	0.701744
-46.800279	-1.989522	2.191859	0.008758	0.701880
-45.722240	-2.086538	2.201856	0.008557	0.702073
-45.968104	-2.042374	2.211853	0.008602	0.702074
-45.940203	-2.048338	2.221850	0.008597	0.702072
-45.921173	-2.022967	2.231846	0.008593	0.702131
-45.103669	-2.050991	2.241843	0.008441	0.702369
-44.816741	-2.102059	2.251840	0.008387	0.702370
-45.049414	-2.060441	2.261837	0.008430	0.702371
-45.281126	-1.967112	2.271834	0.008473	0.702476
-44.165062	-2.061920	2.281830	0.008265	0.702687
-44.279757	-2.039289	2.291827	0.008286	0.702692
-44.258862	-2.041723	2.301824	0.008282	0.702695
-43.483404	-2.054639	2.311821	0.008138	0.702948
-43.554235	-2.013478	2.321818	0.008151	0.703006
-43.276624	-2.063076	2.331814	0.008099	0.703007
-43.316326	-2.027928	2.341811	0.008106	0.703064
-42.408149	-2.051659	2.351808	0.007937	0.703343
-42.337547	-2.063148	2.361805	0.007923	0.703346
-42.595915	-2.017415	2.371802	0.007971	0.703345
-42.169653	-2.018016	2.381798	0.007892	0.703498
-41.678791	-2.036585	2.391795	0.007800	0.703637
-41.555827	-2.058957	2.401792	0.007777	0.703637
-41.478695	-2.073507	2.411789	0.007763	0.703635
-41.108915	-1.985819	2.421786	0.007694	0.703946
-40.740820	-2.048679	2.431782	0.007625	0.703952
-40.620799	-2.068976	2.441779	0.007602	0.703954
-40.422486	-2.026035	2.451776	0.007565	0.704112
-40.016358	-2.024624	2.461773	0.007489	0.704262
-40.001074	-2.027875	2.471770	0.007486	0.704261
-39.746694	-2.057278	2.481766	0.007439	0.704293
-39.156710	-2.013620	2.491763	0.007329	0.704594
-39.011301	-2.041738	2.501760	0.007302	0.704590
-39.171638	-2.011858	2.511757	0.007331	0.704593
-38.752636	-1.982348	2.521754	0.007253	0.704803
-38.225497	-2.033977	2.531750	0.007155	0.704889
-38.138689	-2.049398	2.541747	0.007138	0.704889
-38.019795	-2.021334	2.551744	0.007116	0.704989
-37.354617	-2.028232	2.561741	0.006992	0.705214
-37.203250	-2.056520	2.571738	0.006964	0.705212
-37.445558	-2.013346	2.581734	0.007008	0.705212
-36.723255	-2.017108	2.591731	0.006874	0.705464
-36.380380	-2.047961	2.601728	0.006810	0.705525
-36.627511	-2.004044	2.611725	0.006856	0.705525
-36.373804	-1.986331	2.621722	0.006808	0.705652
-35.300497	-2.072202	2.631718	0.006608	0.705865
-35.539308	-2.028565	2.641715	0.006652	0.705867
-35.417657	-2.049963	2.651712	0.006630	0.705868
-35.202265	-1.992853	2.661709	0.006589	0.706061
-34.815467	-2.028397	2.671706	0.006517	0.706128
-34.928723	-2.005626	2.681702	0.006538	0.706134
-34.520660	-2.000205	2.691699	0.006462	0.706291
-33.816099	-2.048123	2.701696	0.006330	0.706448
-34.037667	-2.008183	2.711693	0.006371	0.706449
-33.939650	-2.009848	2.721690	0.006353	0.706481
-33.247479	-1.998186	2.731686	0.006224	0.706753
-32.947746	-2.050469	2.741683	0.006168	0.706755
-33.282743	-1.991983	2.751680	0.006230	0.706753
-32.596650	-1.978831	2.761677	0.006102	0.707026
-32.332273	-1.999352	2.771674	0.006053	0.707079
-32.168293	-2.028214	2.781670	0.006022	0.707080
-31.959104	-2.001324	2.791667	0.005983	0.707210
-30.958754	-2.095542	2.801664	0.005797	0.707379
-31.293400	-2.036149	2.811661	0.005859	0.707379
-31.166782	-2.060103	2.821658	0.005835	0.707376
-30.831495	-2.003615	2.831654	0.005772	0.707610
-30.303747	-2.053248	2.841651	0.005674	0.707699
-30.299390	-2.052449	2.851648	0.005673	0.707703
-30.281000	-2.032564	2.861645	0.005669	0.707750
-29.531179	-2.035707	2.871642	0.005529	0.708012
-29.407538	-2.057805	2.881638	0.005506	0.708012
-29.360327	-2.065618	2.891635	0.005497	0.708013
-29.308096	-1.970617	2.901632	0.005487	0.708223
-28.781698	-1.998787	2.911629	0.005389	0.708355
-28.667127	-2.020946	2.921626	0.005368	0.708352
-28.778858	-1.966184	2.931622	0.005388	0.708422
-27.827538	-2.025902	2.941619	0.005211	0.708642
-27.631739	-2.060275	2.951616	0.005174	0.708644
-28.012367	-1.992067	2.961613	0.005245	0.708645
-27.214922	-1.992392	2.971610	0.005096	0.708929
-27.106863	-1.996644	2.981606	0.005076	0.708959
-26.860091	-2.040490	2.991603	0.005030	0.708960
-26.900584	-1.948067	3.001600	0.005037	0.709131
-26.145320	-2.012832	3.011597	0.004896	0.709271
-26.241315	-1.996448	3.021594	0.004914	0.709270
-26.184666	-1.978445	3.031590	0.004903	0.709327
-25.132918	-2.027888	3.041587	0.004707	0.709603
-25.164323	-2.022977	3.051584	0.004713	0.709602
-25.129228	-2.031636	3.061581	0.004706	0.709597
-24.878599	-1.981557	3.071578	0.004659	0.709787
-24.272588	-2.035754	3.081574	0.004546	0.709895
-24.325265	-2.025997	3.091571	0.004556	0.709896
-24.436985	-1.985585	3.101568	0.004577	0.709938
-23.238977	-2.059278	3.111565	0.004353	0.710217
-23.549714	-2.002437	3.121562	0.004411	0.710221
-23.478271	-2.015073	3.131558	0.004398	0.710221
-23.088860	-2.005676	3.141555	0.004325	0.710379
-22.544440	-2.023257	3.151552	0.004223	0.710538
-22.576533	-2.018498	3.161549	0.004229	0.710537
-22.714214	-1.985962	3.171546	0.004255	0.710553
-21.801743	-1.988906	3.181542	0.004084	0.710872
-21.534497	-2.034711	3.191539	0.004034	0.710876
-21.767877	-1.991617	3.201536	0.004078	0.710879
-21.343638	-1.996882	3.211533	0.003999	0.711020
-21.111032	-1.977108	3.221530	0.003955	0.711143
-20.789803	-2.033667	3.231526	0.003895	0.711144
-20.818382	-2.009013	3.241523	0.003900	0.711184
-20.302445	-1.962260	3.251520	0.003804	0.711461
-19.998885	-2.016805	3.261517	0.003747	0.711460
-20.216301	-1.979886	3.271514	0.003788	0.711457
-19.463314	-1.984762	3.281510	0.003647	0.711715
-19.277754	-1.992880	3.291507	0.003612	0.711765
-19.091728	-2.025343	3.301504	0.003578	0.711767
-18.939790	-1.986734	3.311501	0.003549	0.711898
-18.315310	-2.000548	3.321498	0.003433	0.712093
-18.242242	-2.013354	3.331494	0.003419	0.712094
-18.339079	-1.995728	3.341491	0.003437	0.712095
-17.597303	-1.994986	3.351488	0.003298	0.712360
-17.286500	-2.034968	3.361485	0.003240	0.712391
-17.321691	-2.029032	3.371482	0.003247	0.712391
-17.332160	-1.983674	3.381478	0.003248	0.712478
-16.706599	-1.978477	3.391475	0.003132	0.712710
-16.403958	-2.030380	3.401472	0.003075	0.712715
-16.521152	-2.010266	3.411469	0.003097	0.712713
-16.060730	-1.952591	3.421466	0.003011	0.712992
-15.452064	-2.044332	3.431462	0.002897	0.713026
-15.551070	-2.026673	3.441459	0.002916	0.713026
-15.403788	-2.007731	3.451456	0.002888	0.713116
-14.509609	-2.041909	3.461453	0.002721	0.713365
-14.577676	-2.031374	3.471450	0.002734	0.713363
-14.589211	-2.030165	3.481446	0.002736	0.713361
-14.570677	-1.947941	3.491443	0.002732	0.713532
-13.532371	-2.070381	3.501440	0.002539	0.713656
-13.983271	-1.991953	3.511437	0.002622	0.713653
-13.758447	-2.016385	3.521434	0.002580	0.713684
-12.901140	-2.025204	3.531430	0.002421	0.713971
-13.114934	-1.987370	3.541427	0.002460	0.713971
-12.666153	-2.065931	3.551424	0.002377	0.713974
-12.563714	-1.998106	3.561421	0.002357	0.714145
-12.058272	-2.020707	3.571418	0.002263	0.714280
-12.137889	-2.008589	3.581414	0.002278	0.714276
-12.165000	-1.984854	3.591411	0.002282	0.714314
-10.888913	-2.063260	3.601408	0.002045	0.714610
-11.031823	-2.038372	3.611405	0.002071	0.714609
-10.592482	-2.117293	3.621402	0.001989	0.714608
-10.587638	-2.117625	3.631398	0.001988	0.714610
-10.189169	-2.042170	3.641395	0.001914	0.714901
-9.946706	-2.078730	3.651392	0.001868	0.714914
-9.793926	-2.106835	3.661389	0.001840	0.714913
-9.898087	-2.074239	3.671386	0.001859	0.714941
-9.085890	-2.072377	3.681382	0.001707	0.715232
-8.718037	-2.137141	3.691379	0.001639	0.715234
-8.883901	-2.106116	3.701376	0.001670	0.715237
-9.105352	-2.026575	3.711373	0.001711	0.715317
-7.957826	-2.113417	3.721370	0.001497	0.715551
-8.122168	-2.084792	3.731366	0.001527	0.715550
-8.193640	-2.070306	3.741363	0.001540	0.715553
-7.506167	-2.092420	3.751360	0.001412	0.715753
-7.111986	-2.095465	3.761357	0.001338	0.715886
-6.997265	-2.115921	3.771354	0.001317	0.715886
-7.116478	-2.095573	3.781350	0.001339	0.715885
-6.451247	-2.130281	3.791347	0.001215	0.716051
-6.336377	-2.105435	3.801344	0.001193	0.716142
-6.224107	-2.125849	3.811341	0.001172	0.716141
-6.196234	-2.125114	3.821338	0.001167	0.716153
-5.646575	-2.071751	3.831334	0.001064	0.716453
-5.503621	-2.096367	3.841331	0.001038	0.716455
-5.229747	-2.144028	3.851328	0.000986	0.716457
-5.226055	-2.054070	3.861325	0.000985	0.716637
-4.486793	-2.124810	3.871322	0.000848	0.716758
-4.884482	-2.053872	3.881318	0.000921	0.716759
-4.562855	-2.070073	3.891315	0.000861	0.716840
-3.560608	-2.122179	3.901312	0.000675	0.717091
-3.622896	-2.112131	3.911309	0.000686	0.717089
-3.597797	-2.118953	3.921306	0.000681	0.717085
-3.369873	-2.055890	3.931302	0.000639	0.717290
-2.675448	-2.132966	3.941299	0.000509	0.717383
-2.970609	-2.080135	3.951296	0.000564	0.717383
-2.789729	-2.072452	3.961293	0.000530	0.717463
-1.956573	-2.095345	3.971290	0.000375	0.717711
-1.836137	-2.117409	3.981286	0.000352	0.717710
-1.781278	-2.127319	3.991283	0.000342	0.717710
-1.902803	-2.001839	4.001280	0.000364	0.717916
-1.345443	-2.045592	4.011277	0.000260	0.718026
-1.414125	-2.035634	4.021274	0.000273	0.718022
-1.310636	-1.948206	4.031270	0.000253	0.718231
-1.130653	-1.916289	4.041267	0.000219	0.718358
-1.265098	-1.891175	4.051264	0.000244	0.718361
-1.111873	-1.774902	4.061261	0.000215	0.718644
-0.850817	-1.822011	4.071258	0.000167	0.718643
-1.213146	-1.641189	4.081254	0.000234	0.718873
-0.870657	-1.656535	4.091251	0.000170	0.718964
-0.537790	-1.600902	4.101248	0.000108	0.719191
-0.427629	-1.577069	4.111245	0.000087	0.719277
-0.391783	-1.461786	4.121242	0.000080	0.719517
-0.509166	-1.398875	4.131238	0.000102	0.719600
-0.459969	-1.262117	4.141235	0.000092	0.719887
-0.544521	-1.179604	4.151232	0.000108	0.720021
-0.334575	-1.112779	4.161229	0.000068	0.720226
-0.142693	-1.014444	4.171226	0.000032	0.720487
-0.246987	-0.906877	4.181222	0.000052	0.720663
-0.058261	-0.831134	4.191219	0.000016	0.720878
0.006291	-0.721564	4.201216	0.000004	0.721117
-0.003021	-0.613427	4.211213	0.000005	0.721327
-0.111365	-0.477406	4.221210	0.000025	0.721557
-0.105210	-0.348693	4.231206	0.000024	0.721812
0.033286	-0.231921	4.241203	-0.000002	0.722090
-0.134355	-0.059429	4.251200	0.000029	0.722371
0.000000	0.115275	4.261197	0.000003	0.722761

-0.092961	0.768559	4.266202	0.000020	0.724010
0.266289	1.963231	4.271206	-0.000047	0.726471
0.590068	3.775901	4.276211	-0.000109	0.730114
0.669096	6.174134	4.281216	-0.000125	0.734785
1.238925	8.998542	4.286221	-0.000233	0.740412
1.681848	12.332348	4.291226	-0.000318	0.746920
2.085962	16.120024	4.296230	-0.000396	0.754213
2.464368	20.328775	4.301235	-0.000469	0.762212
2.881279	24.921008	4.306240	-0.000550	0.770846
3.206765	29.901554	4.311245	-0.000614	0.780061
3.574551	35.224897	4.316250	-0.000686	0.789797
3.947260	40.851672	4.321254	-0.000759	0.799955
4.442846	46.774081	4.326259	-0.000855	0.810540
4.698846	53.004128	4.331264	-0.000907	0.821447
5.560090	59.411843	4.336269	-0.001072	0.832695
6.285954	66.063945	4.341274	-0.001211	0.844164
6.657722	73.004037	4.346278	-0.001285	0.855852
7.065565	80.147038	4.351283	-0.001366	0.867724
7.521132	87.456286	4.356288	-0.001456	0.879718
8.540975	94.844450	4.361293	-0.001650	0.891833
9.690530	102.388620	4.366298	-0.001869	0.904066
10.609370	110.122342	4.371302	-0.002046	0.916365
11.796073	117.942772	4.376307	-0.002272	0.928705
12.561368	125.951691	4.381312	-0.002420	0.941056
13.208099	134.094521	4.386317	-0.002546	0.953414
14.028112	142.285954	4.391322	-0.002704	0.965730
14.797265	150.577419	4.396326	-0.002852	0.978022
15.443251	158.974114	4.401331	-0.002978	0.990281
16.466693	167.331624	4.406336	-0.003174	1.002427
17.080789	175.809679	4.411341	-0.003294	1.014496
18.077525	184.263535	4.416346	-0.003485	1.026481
18.883803	192.790067	4.421350	-0.003641	1.038382
19.469342	201.393945	4.426355	-0.003756	1.050200
20.352986	209.960859	4.431360	-0.003926	1.061905
20.844816	218.633432	4.436365	-0.004023	1.073533
21.554305	227.255203	4.441370	-0.004161	1.085018
21.968531	235.940134	4.446374	-0.004244	1.096399
22.476210	244.607101	4.451379	-0.004344	1.107660
23.270772	253.220440	4.456384	-0.004498	1.118802
23.960027	261.858592	4.461389	-0.004632	1.129842
24.388515	270.542621	4.466394	-0.004718	1.140776
25.469055	279.124904	4.471398	-0.004925	1.151618
27.098163	287.619907	4.476403	-0.005234	1.162367
27.492055	296.300357	4.481408	-0.005313	1.172986
27.779136	304.974153	4.486413	-0.005372	1.183479
28.584017	313.567917	4.491418	-0.005527	1.193889
29.300752	322.134796	4.496422	-0.005667	1.204160
29.966153	330.728365	4.501427	-0.005796	1.214365
30.720712	339.272940	4.506432	-0.005942	1.224445
31.288602	347.872236	4.511437	-0.006054	1.234469
31.685394	356.450073	4.516442	-0.006133	1.244354
32.353747	364.969469	4.521446	-0.006263	1.254147
33.290880	373.440704	4.526451	-0.006444	1.263861
33.607511	382.007508	4.531456	-0.006508	1.273490
34.112617	390.513220	4.536461	-0.006608	1.283014
34.481983	399.042583	4.541466	-0.006682	1.292469
35.103524	407.488546	4.546470	-0.006804	1.301810
35.690850	416.022394	4.551475	-0.006919	1.311173
36.253540	424.501981	4.556480	-0.007029	1.320407
36.796305	432.911671	4.561485	-0.007136	1.329499
37.207541	441.352380	4.566490	-0.007218	1.338538
37.661085	449.754347	4.571494	-0.007308	1.347483
38.183204	458.162833	4.576499	-0.007411	1.356387
38.666399	466.532618	4.581504	-0.007506	1.365186
39.368967	474.895916	4.586509	-0.007642	1.373960
40.041174	483.246682	4.591514	-0.007773	1.382659
40.427481	491.637308	4.596518	-0.007851	1.391297
41.157156	499.969059	4.601523	-0.007992	1.399878
41.664508	508.303648	4.606528	-0.008092	1.408373
42.423246	516.614240	4.611533	-0.008239	1.416835
42.886341	524.951984	4.616538	-0.008331	1.425224
43.023790	533.352910	4.621542	-0.008362	1.433573
43.513258	541.655009	4.626547	-0.008458	1.441834
44.026740	549.962867	4.631552	-0.008560	1.450057
44.510574	558.275345	4.636557	-0.008655	1.458233
45.147245	566.549045	4.641562	-0.008779	1.466351
45.910032	574.855338	4.646566	-0.008927	1.474474
46.616679	583.110402	4.651571	-0.009064	1.482495
47.025903	591.405312	4.656576	-0.009145	1.490464
47.487700	599.695028	4.661581	-0.009237	1.498394
48.077876	607.945305	4.666586	-0.009352	1.506264
48.406477	616.245157	4.671590	-0.009419	1.514100
48.989391	624.485711	4.676595	-0.009533	1.521879
49.543275	632.724726	4.681600	-0.009642	1.529612
49.621389	641.059911	4.686605	-0.009662	1.537323
50.275696	649.268573	4.691610	-0.009789	1.544966
50.856522	657.513196	4.696614	-0.009903	1.552592
51.255849	665.771238	4.701619	-0.009982	1.560167
51.482086	674.027268	4.706624	-0.010030	1.567677
51.945632	682.266349	4.711629	-0.010122	1.575172
52.232535	690.519682	4.716634	-0.010181	1.582617
52.616684	698.741777	4.721638	-0.010258	1.590014
53.137562	706.958144	4.726643	-0.010360	1.597391
53.415863	715.175706	4.731648	-0.010417	1.604700
53.967802	723.377450	4.736653	-0.010526	1.612001
54.409294	731.592455	4.741658	-0.010613	1.619265
54.818945	739.786358	4.746662	-0.010695	1.626473
55.280244	748.049744	4.751667	-0.010786	1.633717
55.615928	756.234783	4.756672	-0.010854	1.640844
56.092303	764.409789	4.761677	-0.010948	1.647950
56.476813	772.623970	4.766682	-0.011025	1.655047
57.012736	780.768279	4.771686	-0.011131	1.662074
57.686527	788.934434	4.776691	-0.011261	1.669109
57.972349	797.153007	4.781696	-0.011320	1.676106
58.311387	805.337184	4.786701	-0.011389	1.683052
58.805944	813.511785	4.791706	-0.011486	1.689982
59.155139	821.712239	4.796710	-0.011557	1.696886
59.227981	829.936590	4.801715	-0.011576	1.703746
59.356364	838.153776	4.806720	-0.011605	1.710579
59.764161	846.319501	4.811725	-0.011686	1.717379
60.399782	854.435479	4.816730	-0.011810	1.724141
60.876594	862.576506	4.821734	-0.011904	1.730875
61.294829	870.757609	4.826739	-0.011988	1.737609
61.765109	878.895269	4.831744	-0.012080	1.744288
62.096194	887.078875	4.836749	-0.012148	1.750961
62.317437	895.278872	4.841754	-0.012194	1.757608
62.790910	903.395161	4.846758	-0.012288	1.764194
63.233903	911.566944	4.851763	-0.012376	1.770797
63.464867	919.753513	4.856768	-0.012424	1.777359
63.972015	927.876151	4.861773	-0.012524	1.783881
64.313805	936.075437	4.866778	-0.012593	1.790420
64.922473	944.216341	4.871782	-0.012712	1.796921
65.502282	952.337141	4.876787	-0.012825	1.803379
65.901468	960.464890	4.881792	-0.012905	1.809798
66.342196	968.623298	4.886797	-0.012992	1.816222
66.438306	976.798289	4.891802	-0.013016	1.822596
66.850375	984.920277	4.896806	-0.013098	1.828944
67.286878	993.062082	4.901811	-0.013184	1.835287
67.537598	1001.199316	4.906816	-0.013236	1.841584
68.066388	1009.302637	4.911821	-0.013340	1.847866
68.470159	1017.465679	4.916826	-0.013421	1.854157
68.802299	1025.583710	4.921830	-0.013488	1.860384
69.409109	1033.695932	4.926835	-0.013606	1.866618
69.851401	1041.854774	4.931840	-0.013694	1.872847
70.118872	1050.005706	4.936845	-0.013749	1.879029
70.257000	1058.153767	4.941850	-0.013781	1.885174
70.760614	1066.247545	4.946854	-0.013880	1.891299
71.343979	1074.366390	4.951859	-0.013994	1.897433
71.371550	1082.527504	4.956864	-0.014004	1.903516
71.757694	1090.663196	4.961869	-0.014082	1.909600
72.184010	1098.783005	4.966874	-0.014166	1.915658
72.302076	1106.921875	4.971878	-0.014194	1.921676
72.523127	1115.053207	4.976883	-0.014240	1.927681
72.992501	1123.159688	4.981888	-0.014333	1.933677
73.538254	1131.240697	4.986893	-0.014440	1.939644
73.570358	1139.410979	4.991898	-0.014451	1.945601
74.234840	1147.494223	4.996902	-0.014580	1.951546
75.121662	1155.560312	5.001907	-0.014751	1.957484
75.243075	1163.691557	5.006912	-0.014779	1.963369
75.402865	1171.823776	5.011917	-0.014814	1.969240
75.916168	1179.928080	5.016922	-0.014915	1.975112
76.308137	1188.012568	5.021926	-0.014993	1.980939
76.767318	1196.128950	5.026931	-0.015084	1.986779
77.195340	1204.253596	5.031936	-0.015169	1.992604
77.416592	1212.365003	5.036941	-0.015216	1.998381
77.547414	1220.504437	5.041946	-0.015246	2.004152
77.833754	1228.592111	5.046950	-0.015304	2.009886
78.522619	1236.677604	5.051955	-0.015438	2.015643
79.057331	1244.748713	5.056960	-0.015543	2.021358
79.235585	1252.888107	5.061965	-0.015581	2.027068
79.774912	1261.003024	5.066970	-0.015687	2.032781
80.186939	1269.084867	5.071974	-0.015769	2.038443
80.592923	1277.175314	5.076979	-0.015850	2.044094
81.008653	1285.273273	5.081984	-0.015933	2.049735
81.197843	1293.403971	5.086989	-0.015974	2.055361
81.367833	1301.522417	5.091994	-0.016011	2.060961
81.635685	1309.615289	5.096998	-0.016066	2.066537
82.065905	1317.725524	5.102003	-0.016152	2.072127
82.476625	1325.799214	5.107008	-0.016233	2.077675
82.571950	1333.904429	5.112013	-0.016256	2.083198
83.084481	1341.991565	5.117018	-0.016357	2.088736
83.432266	1350.093311	5.122022	-0.016427	2.094252
84.029174	1358.152798	5.127027	-0.016544	2.099749
84.389085	1366.240565	5.132032	-0.016616	2.105228
84.471145	1374.415712	5.137037	-0.016637	2.110725
84.753220	1382.557928	5.142042	-0.016695	2.116204
84.845449	1390.621306	5.147046	-0.016717	2.121598
85.191314	1398.687777	5.152051	-0.016787	2.127005
85.619136	1406.753624	5.157056	-0.016872	2.132405
85.691756	1414.869334	5.162061	-0.016891	2.137791
86.215330	1422.915383	5.167066	-0.016994	2.143160
86.422005	1431.011047	5.172070	-0.017038	2.148519
86.706438	1439.125240	5.177075	-0.017096	2.153883
86.969775	1447.196211	5.182080	-0.017150	2.159204
87.483572	1455.228660	5.187085	-0.017251	2.164509
87.847779	1463.331484	5.192090	-0.017325	2.169834
88.189429	1471.419313	5.197094	-0.017394	2.175134
88.892630	1479.471457	5.202099	-0.017530	2.180430
89.122142	1487.560263	5.207104	-0.017578	2.185694
89.360108	1495.690518	5.212109	-0.017628	2.190973
89.714316	1503.794573	5.217114	-0.017699	2.196233
90.029583	1511.849268	5.222118	-0.017763	2.201445
90.163179	1519.942590	5.227123	-0.017793	2.206653
90.473223	1528.024434	5.232128	-0.017856	2.211857
90.960654	1536.085927	5.237133	-0.017953	2.217051
91.502403	1544.141412	5.242138	-0.018059	2.222235
91.575189	1552.243306	5.247142	-0.018078	2.227394
91.953907	1560.337703	5.252147	-0.018154	2.232563
92.263808	1568.413371	5.257152	-0.018217	2.237703
92.215276	1576.511877	5.262157	-0.018213	2.242813
92.657984	1584.568503	5.267162	-0.018301	2.247929
92.888269	1592.672153	5.272166	-0.018349	2.253043
93.307341	1600.721050	5.277171	-0.018432	2.258129
93.733173	1608.775225	5.282176	-0.018517	2.263206
93.938480	1616.876385	5.287181	-0.018561	2.268283
94.324071	1625.024060	5.292186	-0.018638	2.273392
94.562544	1633.060111	5.297190	-0.018688	2.278408
94.929539	1641.098064	5.302195	-0.018761	2.283425
95.211733	1649.163386	5.307200	-0.018819	2.288441
95.309646	1657.262625	5.312205	-0.018843	2.293451
95.987210	1665.292844	5.317210	-0.018974	2.298456
96.233545	1673.352483	5.322214	-0.019025	2.303432
96.539301	1681.435340	5.327219	-0.019088	2.308417
96.907286	1689.514351	5.332224	-0.019162	2.313394
97.238435	1697.567201	5.337229	-0.019229	2.318340
97.530193	1705.650559	5.342234	-0.019288	2.323292
97.482953	1713.742870	5.347238	-0.019285	2.328210
97.935516	1721.811518	5.352243	-0.019374	2.333145
98.422802	1729.854666	5.357248	-0.019470	2.338057
98.517184	1737.929883	5.362253	-0.019493	2.342945
98.776916	1746.020354	5.367258	-0.019547	2.347846
99.101546	1754.090834	5.372262	-0.019613	2.352730
99.730683	1762.126490	5.377267	-0.019735	2.357607
99.940288	1770.186049	5.382272	-0.019780	2.362455
100.107797	1778.263025	5.387277	-0.019816	2.367300
100.663880	1786.315372	5.392282	-0.019925	2.372151
100.850107	1794.409368	5.397286	-0.019965	2.376988
101.034048	1802.471665	5.402291	-0.020005	2.381795
101.503258	1810.516376	5.407296	-0.020098	2.386605
101.786431	1818.597515	5.412301	-0.020156	2.391412
101.939590	1826.702434	5.417306	-0.020190	2.396213
102.282711	1834.727631	5.422310	-0.020259	2.400973
102.587753	1842.797425	5.427315	-0.020321	2.405746
102.639517	1850.885755	5.432320	-0.020336	2.410501
103.159074	1858.934102	5.437325	-0.020438	2.415259
103.576660	1866.973468	5.442330	-0.020521	2.419995
103.764731	1875.030892	5.447334	-0.020561	2.424714
103.923011	1883.132217	5.452339	-0.020596	2.429448
104.139150	1891.288026	5.457344	-0.020642	2.434208
104.466091	1899.287605	5.462349	-0.020708	2.438876
104.713182	1907.331314	5.467354	-0.020759	2.443556
105.085931	1915.355178	5.472358	-0.020834	2.448224
105.238925	1923.449169	5.477363	-0.020868	2.452907
105.543878	1931.492169	5.482368	-0.020930	2.457563
105.622895	1939.556277	5.487373	-0.020950	2.462205
105.924516	1947.606036	5.492378	-0.021012	2.466847
106.010916	1955.688328	5.497382	-0.021033	2.471483
106.538054	1963.728446	5.502387	-0.021137	2.476119
106.621199	1971.791896	5.507392	-0.021157	2.480727
106.910672	1979.820833	5.512397	-0.021217	2.485321
107.354388	1987.892639	5.517402	-0.021305	2.489943
107.634607	1995.936473	5.522406	-0.021362	2.494528
108.014187	2003.995964	5.527411	-0.021438	2.499121
108.118732	2012.066241	5.532416	-0.021463	2.503691
108.358956	2020.125821	5.537421	-0.021513	2.508257
108.677448	2028.232057	5.542426	-0.021578	2.512846
108.790310	2036.281935	5.547430	-0.021604	2.517380
109.057390	2044.312700	5.552435	-0.021659	2.521907
109.491648	2052.326610	5.557440	-0.021745	2.526428
109.552165	2060.421684	5.562445	-0.021762	2.530959
109.866408	2068.503384	5.567450	-0.021826	2.535493
110.049880	2076.532878	5.572454	-0.021865	2.539981
110.771203	2084.517755	5.577459	-0.022005	2.544473
110.935283	2092.608870	5.582464	-0.022041	2.548978
111.273062	2100.668680	5.587469	-0.022109	2.553469
111.714176	2108.700151	5.592474	-0.022197	2.557944
111.988686	2116.726316	5.597478	-0.022253	2.562396
112.122460	2124.823223	5.602483	-0.022283	2.566870
112.564791	2132.888606	5.607488	-0.022371	2.571340
112.703434	2140.964189	5.612493	-0.022402	2.575786
113.133754	2149.006597	5.617498	-0.022488	2.580227
113.298992	2157.047627	5.622502	-0.022524	2.584641
113.688866	2165.122368	5.627507	-0.022602	2.589082
113.905924	2173.350531	5.632512	-0.022648	2.593586
114.086229	2181.372007	5.637517	-0.022686	2.597968
114.380929	2189.393155	5.642522	-0.022747	2.602350
114.915069	2197.354432	5.647526	-0.022851	2.606708
114.869949	2205.439762	5.652531	-0.022848	2.611087
115.280572	2213.477420	5.657536	-0.022930	2.615463
115.593815	2221.474058	5.662541	-0.022994	2.619804
115.797534	2229.527556	5.667546	-0.023037	2.624160
115.949722	2237.573077	5.672550	-0.023071	2.628502
116.347163	2245.634286	5.677555	-0.023150	2.632861
116.718478	2253.667481	5.682560	-0.023225	2.637196
116.782213	2261.700052	5.687565	-0.023242	2.641503
117.021194	2269.757555	5.692570	-0.023292	2.645828
117.142806	2277.811187	5.697574	-0.023320	2.650136
117.293613	2285.892013	5.702579	-0.023353	2.654453
117.754813	2293.902940	5.707584	-0.023444	2.658746
118.078082	2301.924525	5.712589	-0.023510	2.663030
118.321203	2310.000208	5.717594	-0.023560	2.667329
118.617317	2318.063157	5.722598	-0.023621	2.671618
118.946667	2326.121027	5.727603	-0.023688	2.675900
119.203237	2334.149340	5.732608	-0.023741	2.680155
119.380507	2342.165788	5.737613	-0.023779	2.684392
119.750960	2350.228063	5.742618	-0.023853	2.688658
119.862223	2358.304322	5.747622	-0.023879	2.692908
120.135478	2366.352452	5.752627	-0.023936	2.697147
120.497907	2374.379417	5.757632	-0.024008	2.701374
120.597849	2382.411860	5.762637	-0.024032	2.705581
120.901874	2390.489849	5.767642	-0.024094	2.709817
121.032484	2398.547482	5.772646	-0.024124	2.714026
121.377591	2406.590867	5.777651	-0.024194	2.718233
121.655347	2414.606860	5.782656	-0.024251	2.722416
121.779616	2422.653635	5.787661	-0.024279	2.726599
122.158255	2430.701288	5.792666	-0.024355	2.730792
122.473552	2438.747311	5.797670	-0.024419	2.734973
122.675522	2446.798702	5.802675	-0.024462	2.739144
122.762989	2454.843928	5.807680	-0.024483	2.743298
123.010142	2462.890428	5.812685	-0.024535	2.747456
123.324854	2471.002678	5.817690	-0.024599	2.751646
123.457311	2479.071646	5.822694	-0.024629	2.755796
123.849730	2487.063169	5.827699	-0.024707	2.759916
124.211854	2495.061263	5.832704	-0.024780	2.764031
124.392183	2503.094624	5.837709	-0.024819	2.768147
124.758150	2511.162423	5.842714	-0.024892	2.772285
124.979024	2519.228163	5.847718	-0.024939	2.776408
125.126012	2527.262437	5.852723	-0.024972	2.780504
125.364525	2535.285081	5.857728	-0.025021	2.784593
125.742746	2543.317593	5.862733	-0.025097	2.788690
126.177872	2551.367873	5.867738	-0.025183	2.792793
126.149739	2559.427677	5.872742	-0.025183	2.796868
126.612311	2567.451156	5.877747	-0.025275	2.800946
126.911206	2575.486282	5.882752	-0.025336	2.805016
127.011216	2583.533209	5.887757	-0.025360	2.809073
127.308802	2591.616955	5.892762	-0.025421	2.813155
127.517148	2599.624543	5.897766	-0.025465	2.817187
127.676462	2607.684869	5.902771	-0.025500	2.821238
127.693553	2615.750685	5.907776	-0.025508	2.825277
127.963577	2623.782288	5.912781	-0.025564	2.829307
128.383873	2631.844663	5.917786	-0.025647	2.833356
128.602836	2639.865270	5.922790	-0.025694	2.837366
128.694231	2647.899300	5.927795	-0.025716	2.841371
128.865939	2655.925552	5.932800	-0.025753	2.845370
128.894180	2663.964344	5.937805	-0.025764	2.849362
129.367013	2672.016473	5.942810	-0.025857	2.853379
129.479139	2680.044563	5.947814	-0.025883	2.857359
129.870347	2688.079013	5.952819	-0.025962	2.861352
130.082033	2696.112822	5.957824	-0.026006	2.865329
130.307885	2704.144917	5.962829	-0.026054	2.869301
130.613605	2712.232636	5.967834	-0.026116	2.873299
130.678640	2720.257030	5.972838	-0.026133	2.877246
131.076678	2728.275018	5.977843	-0.026213	2.881204
131.464913	2736.305348	5.982848	-0.026290	2.885161
131.656825	2744.348992	5.987853	-0.026332	2.889109
132.038269	2752.418479	5.992858	-0.026408	2.893074
132.439984	2760.415083	5.997862	-0.026488	2.897000
132.667073	2768.483111	6.002867	-0.026536	2.900945
132.795365	2776.529536	6.007872	-0.026565	2.904869
132.824215	2784.574115	6.012877	-0.026576	2.908781
133.370949	2792.687043	6.017882	-0.026683	2.912749
133.502729	2800.732602	6.022886	-0.026713	2.916657
133.723303	2808.723149	6.027891	-0.026759	2.920538
133.995040	2816.707214	6.032896	-0.026815	2.924413
134.014862	2824.759980	6.037901	-0.026824	2.928303
134.138324	2832.846491	6.042906	-0.026852	2.932209
134.669766	2840.818961	6.047910	-0.026957	2.936076
134.852814	2848.864817	6.052915	-0.026996	2.939956
134.890304	2856.903392	6.057920	-0.027008	2.943819
135.003632	2864.943681	6.062925	-0.027035	2.947682
135.588089	2872.982735	6.067930	-0.027149	2.951563
135.694934	2881.033998	6.072934	-0.027174	2.955421
135.897497	2889.039757	6.077939	-0.027217	2.959257
136.335904	2897.073191	6.082944	-0.027304	2.963113
136.273206	2905.124616	6.087949	-0.027298	2.966947
136.455317	2913.194968	6.092954	-0.027337	2.970797
136.840547	2921.223264	6.097958	-0.027414	2.974633
136.976108	2929.266432	6.102963	-0.027445	2.978458
137.153769	2937.298398	6.107968	-0.027483	2.982275
137.318035	2945.325025	6.112973	-0.027519	2.986083
137.815306	2953.359644	6.117978	-0.027617	2.989908
138.026890	2961.426520	6.122982	-0.027662	2.993728
138.261990	2969.454968	6.127987	-0.027711	2.997527
138.719194	2977.473576	6.132992	-0.027801	3.001327
138.976895	2985.463212	6.137997	-0.027854	3.005099
139.249568	2993.516633	6.143002	-0.027911	3.008896
139.328727	3001.577414	6.148006	-0.027931	3.012683
139.752384	3009.614919	6.153011	-0.028015	3.016471
139.952602	3017.646773	6.158016	-0.028057	3.020240
139.979526	3025.680153	6.163021	-0.028068	3.023997
140.399833	3033.709276	6.168026	-0.028151	3.027767
140.647662	3041.749841	6.173030	-0.028203	3.031529
140.849899	3049.799900	6.178035	-0.028246	3.035288
141.076434	3057.794406	6.183040	-0.028293	3.039018
141.325808	3065.820027	6.188045	-0.028345	3.042758
141.490602	3073.890655	6.193050	-0.028381	3.046511
141.660255	3081.908814	6.198054	-0.028418	3.050236
141.896107	3089.980670	6.203059	-0.028467	3.053983
142.228753	3098.002623	6.208064	-0.028535	3.057708
142.039288	3106.048161	6.213069	-0.028505	3.061414
142.565246	3114.053164	6.218074	-0.028608	3.065131
142.746924	3122.101298	6.223078	-0.028647	3.068847
142.749320	3130.226454	6.228083	-0.028653	3.072585
143.008510	3138.284395	6.233088	-0.028707	3.076300
143.297516	3146.225991	6.238093	-0.028766	3.079958
143.490642	3154.255730	6.243098	-0.028807	3.083648
143.754031	3162.274439	6.248102	-0.028861	3.087332
144.032796	3170.308827	6.253107	-0.028918	3.091019
144.316256	3178.364112	6.258112	-0.028977	3.094711
144.311739	3186.375971	6.263117	-0.028981	3.098366
144.712711	3194.397716	6.268122	-0.029061	3.102040
144.960738	3202.404012	6.273126	-0.029113	3.105695
145.047589	3210.456608	6.278131	-0.029134	3.109359
145.383045	3218.536597	6.283136	-0.029202	3.113043
145.569352	3226.549582	6.288141	-0.029242	3.116686
145.922316	3234.571333	6.293146	-0.029313	3.120336
145.932438	3242.595948	6.298150	-0.029320	3.123967
146.367294	3250.596142	6.303155	-0.029406	3.127602
146.736703	3258.638637	6.308160	-0.029481	3.131248
146.823635	3266.701939	6.313165	-0.029502	3.134888
147.029870	3274.740026	6.318170	-0.029546	3.138517
147.421048	3282.749216	6.323174	-0.029624	3.142137
147.562819	3290.795780	6.328179	-0.029656	3.145758
147.766476	3298.851904	6.333184	-0.029699	3.149383
147.914847	3306.913758	6.338189	-0.029732	3.153003
148.253311	3314.953872	6.343194	-0.029800	3.156618
148.214296	3322.952790	6.348198	-0.029798	3.160193
148.390537	3330.960135	6.353203	-0.029836	3.163778
148.684425	3338.981360	6.358208	-0.029896	3.167370
148.940395	3347.001493	6.363213	-0.029949	3.170955
149.086948	3355.103847	6.368218	-0.029982	3.174569
149.162995	3363.095859	6.373222	-0.030002	3.178126
149.454638	3371.118343	6.378227	-0.030061	3.181702
149.682813	3379.145533	6.383232	-0.030109	3.185273
149.974812	3387.160236	6.388237	-0.030169	3.188838
150.094266	3395.242880	6.393242	-0.030196	3.192421
150.210546	3403.285524	6.398246	-0.030223	3.195982
150.679995	3411.263999	6.403251	-0.030316	3.199526
150.968947	3419.303389	6.408256	-0.030375	3.203085
151.057546	3427.335414	6.413261	-0.030397	3.206628
151.395909	3435.378304	6.418266	-0.030465	3.210183
151.738094	3443.399376	6.423270	-0.030534	3.213724
151.768689	3451.446723	6.428275	-0.030545	3.217260
151.900447	3459.509814	6.433280	-0.030575	3.220803
152.164041	3467.466147	6.438285	-0.030630	3.224301
152.570172	3475.522091	6.443290	-0.030711	3.227845
152.589483	3483.582502	6.448294	-0.030720	3.231370
153.066913	3491.638361	6.453299	-0.030814	3.234909
153.377160	3499.626481	6.458304	-0.030877	3.238407
153.524224	3507.642841	6.463309	-0.030910	3.241907
153.659328	3515.674073	6.468314	-0.030940	3.245410
153.821471	3523.663435	6.473318	-0.030975	3.248891
154.000292	3531.753383	6.478323	-0.031014	3.252413
154.092046	3539.827097	6.483328	-0.031037	3.255920
154.220060	3547.780867	6.488333	-0.031066	3.259374
154.739764	3555.806068	6.493338	-0.031168	3.262870
155.022952	3563.834325	6.498342	-0.031226	3.266354
155.050222	3571.858506	6.503347	-0.031236	3.269822
155.179680	3579.949945	6.508352	-0.031266	3.273320
155.434436	3587.942381	6.513357	-0.031318	3.276777
155.583859	3595.992094	6.518362	-0.031352	3.280250
155.874809	3603.988252	6.523366	-0.031411	3.283702
156.258595	3611.991132	6.528371	-0.031488	3.287157
156.131450	3620.087202	6.533376	-0.031470	3.290628
156.341451	3628.104662	6.538381	-0.031514	3.294075
156.519083	3636.156130	6.543386	-0.031552	3.297532
156.692299	3644.159613	6.548390	-0.031590	3.300964
156.927760	3652.152078	6.553395	-0.031639	3.304390
157.310470	3660.200538	6.558400	-0.031716	3.307843
157.423482	3668.241311	6.563405	-0.031742	3.311278
157.712397	3676.310068	6.568410	-0.031801	3.314728
158.191577	3684.262698	6.573414	-0.031896	3.318132
158.747909	3692.268324	6.578419	-0.032005	3.321558
158.750034	3700.321036	6.583424	-0.032010	3.324980
158.859053	3708.338801	6.588429	-0.032036	3.328387
159.244738	3716.398029	6.593434	-0.032113	3.331819
159.452476	3724.440777	6.598438	-0.032157	3.335234
159.677282	3732.427639	6.603443	-0.032204	3.338622
159.918621	3740.495919	6.608448	-0.032255	3.342041
160.088873	3748.492963	6.613453	-0.032292	3.345424
160.281084	3756.548117	6.618458	-0.032333	3.348830
160.559896	3764.572942	6.623462	-0.032390	3.352222
160.892981	3772.615445	6.628467	-0.032457	3.355620
160.881192	3780.642510	6.633472	-0.032460	3.358995
160.970451	3788.673424	6.638477	-0.032482	3.362373
161.429517	3796.725393	6.643482	-0.032573	3.365769
161.583475	3804.710518	6.648486	-0.032607	3.369122
161.731190	3812.772818	6.653491	-0.032640	3.372505
162.152819	3820.828164	6.658496	-0.032724	3.375890
162.288584	3828.812988	6.663501	-0.032754	3.379233
162.351743	3836.875524	6.668506	-0.032772	3.382602
162.541512	3844.898736	6.673510	-0.032812	3.385956
162.869946	3852.892813	6.678515	-0.032879	3.389300
163.046432	3861.009771	6.683520	-0.032917	3.392686
163.107193	3869.023750	6.688525	-0.032934	3.396021
163.404484	3877.001009	6.693530	-0.032994	3.399346
163.571833	3884.992579	6.698534	-0.033031	3.402670
163.783010	3893.010986	6.703539	-0.033075	3.406003
163.971281	3901.035491	6.708544	-0.033116	3.409334
164.254044	3909.072921	6.713549	-0.033174	3.412670
164.391700	3917.131136	6.718554	-0.033205	3.416007
164.709009	3925.100033	6.723558	-0.033269	3.419310
164.937739	3933.140860	6.728563	-0.033317	3.422636
165.012980	3941.179525	6.733568	-0.033336	3.425953
165.131307	3949.191394	6.738573	-0.033364	3.429257
165.546491	3957.250506	6.743578	-0.033446	3.432587
165.687695	3965.286841	6.748582	-0.033478	3.435895
165.837484	3973.269452	6.753587	-0.033511	3.439179
166.025035	3981.319885	6.758592	-0.033551	3.442488
166.246452	3989.328167	6.763597	-0.033598	3.445778
166.614771	3997.337667	6.768602	-0.033672	3.449070
166.798594	4005.435550	6.773606	-0.033711	3.452389
167.068465	4013.443448	6.778611	-0.033767	3.455671
167.137496	4021.475225	6.783616	-0.033785	3.458953
167.376981	4029.459663	6.788621	-0.033835	3.462218
167.554470	4037.521857	6.793626	-0.033873	3.465509
167.840179	4045.540983	6.798630	-0.033932	3.468784
167.881153	4053.605724	6.803635	-0.033945	3.472066
168.187527	4061.630160	6.808640	-0.034007	3.475337
168.240920	4069.638480	6.813645	-0.034023	3.478590
168.479706	4077.650469	6.818650	-0.034072	3.481847
168.620136	4085.634664	6.823654	-0.034104	3.485087
168.956157	4093.658053	6.828659	-0.034172	3.488346
169.036604	4101.713773	6.833664	-0.034192	3.491607
169.438678	4109.738782	6.838669	-0.034272	3.494863
169.598392	4117.778765	6.843674	-0.034307	3.498114
169.662629	4125.802759	6.848678	-0.034325	3.501352
169.929595	4133.783607	6.853683	-0.034380	3.504577
170.184935	4141.811627	6.858688	-0.034432	3.507817
170.105646	4149.861383	6.863693	-0.034423	3.511052
170.393061	4157.920605	6.868698	-0.034482	3.514299
170.543745	4165.909236	6.873702	-0.034515	3.517511
170.745232	4173.919261	6.878707	-0.034558	3.520731
170.953317	4181.933875	6.883712	-0.034602	3.523949
170.988222	4189.977702	6.888717	-0.034614	3.527170
171.286005	4198.038589	6.893722	-0.034675	3.530404
171.468322	4206.068874	6.898726	-0.034714	3.533618
171.613199	4214.081233	6.903731	-0.034746	3.536822
171.872122	4222.111116	6.908736	-0.034800	3.540033
172.141172	4230.099063	6.913741	-0.034855	3.543225
172.350818	4238.188226	6.918746	-0.034900	3.546452
172.308925	4246.219685	6.923750	-0.034897	3.549646
172.820864	4254.285375	6.928755	-0.034998	3.552867
172.943588	4262.350648	6.933760	-0.035026	3.556073
173.169592	4270.268369	6.938765	-0.035073	3.559221
173.307640	4278.304528	6.943770	-0.035104	3.562410
173.539411	4286.296077	6.948774	-0.035153	3.565582
173.481899	4294.328805	6.953779	-0.035147	3.568758
173.625707	4302.354663	6.958784	-0.035180	3.571935
174.020018	4310.370955	6.963789	-0.035258	3.575113
174.516140	4318.393454	6.968794	-0.035356	3.578293
174.457630	4326.423365	6.973798	-0.035350	3.581457
174.928523	4334.408374	6.978803	-0.035443	3.584616
175.252834	4342.487469	6.983808	-0.035509	3.587805
175.435290	4350.470577	6.988813	-0.035548	3.590949
176.026321	4358.472638	6.993818	-0.035664	3.594109
176.187634	4366.516118	6.998822	-0.035699	3.597271
176.190980	4374.523133	7.003827	-0.035705	3.600411
176.442563	4382.546487	7.008832	-0.035757	3.603562
176.547366	4390.578682	7.013837	-0.035782	3.606709
176.945749	4398.602644	7.018842	-0.035862	3.609859
177.151920	4406.644246	7.023846	-0.035905	3.613007
177.490302	4414.685205	7.028851	-0.035974	3.616156
177.805374	4422.675728	7.033856	-0.036038	3.619282
177.895631	4430.705961	7.038861	-0.036060	3.622414
178.251861	4438.718909	7.043866	-0.036131	3.625544
178.585242	4446.747773	7.048870	-0.036199	3.628677
178.511634	4454.813750	7.053875	-0.036190	3.631810
178.729483	4462.890504	7.058880	-0.036236	3.634953
178.895614	4470.859630	7.063885	-0.036273	3.638050
179.133148	4478.911241	7.068890	-0.036322	3.641179
179.208159	4486.858559	7.073894	-0.036341	3.644259
179.411561	4494.931299	7.078899	-0.036385	3.647390
179.810371	4502.945974	7.083904	-0.036464	3.650500
179.762893	4511.001446	7.088909	-0.036461	3.653611
179.922757	4519.061757	7.093914	-0.036496	3.656727
180.404828	4527.015599	7.098918	-0.036591	3.659808
180.298839	4535.036529	7.103923	-0.036576	3.662897
180.400511	4543.106102	7.108928	-0.036601	3.666007
180.639742	4551.080758	7.113933	-0.036651	3.669081
180.922920	4559.156755	7.118938	-0.036709	3.672193
181.122368	4567.154282	7.123942	-0.036751	3.675270
181.285992	4575.139842	7.128947	-0.036787	3.678339
181.697730	4583.150630	7.133952	-0.036869	3.681422
182.104790	4591.162111	7.138957	-0.036950	3.684501
182.405275	4599.207132	7.143962	-0.037011	3.687589
182.734644	4607.244879	7.148966	-0.037078	3.690671
183.046172	4615.271061	7.153971	-0.037141	3.693747
183.194760	4623.312330	7.158976	-0.037174	3.696821
183.323019	4631.289658	7.163981	-0.037203	3.699868
183.475249	4639.341702	7.168986	-0.037237	3.702941
183.736344	4647.357340	7.173990	-0.037291	3.706000
183.794936	4655.377281	7.178995	-0.037307	3.709054
183.942881	4663.471181	7.184000	-0.037340	3.712136
184.183384	4671.523982	7.189005	-0.037390	3.715201
184.445119	4679.528704	7.194010	-0.037444	3.718246
184.719980	4687.499745	7.199014	-0.037501	3.721276
184.954605	4695.450318	7.204019	-0.037550	3.724295
185.078276	4703.518447	7.209024	-0.037578	3.727354
185.163183	4711.516486	7.214029	-0.037599	3.730382
185.598523	4719.546775	7.219034	-0.037686	3.733429
185.541351	4727.602538	7.224038	-0.037680	3.736470
185.673160	4735.590884	7.229043	-0.037710	3.739489
186.075880	4743.603521	7.234048	-0.037790	3.742520
186.165039	4751.636664	7.239053	-0.037812	3.745549
186.203396	4759.704413	7.244058	-0.037825	3.748588
186.414535	4767.722325	7.249062	-0.037869	3.751609
186.561590	4775.752436	7.254067	-0.037902	3.754632
186.655911	4783.796507	7.259072	-0.037925	3.757655
186.833159	4791.755448	7.264077	-0.037963	3.760646
187.036394	4799.775015	7.269082	-0.038007	3.763659
187.155125	4807.839618	7.274086	-0.038034	3.766683
187.152465	4815.852272	7.279091	-0.038039	3.769683
187.348728	4823.910137	7.284096	-0.038081	3.772702
187.807722	4831.930208	7.289101	-0.038171	3.775710
187.765147	4839.921146	7.294106	-0.038169	3.778694
187.881378	4847.951498	7.299110	-0.038196	3.781694
188.176440	4855.910541	7.304115	-0.038256	3.784668
188.274145	4863.990895	7.309120	-0.038280	3.787681
188.584560	4871.994575	7.314125	-0.038343	3.790668
188.981842	4880.067546	7.319130	-0.038422	3.793680
189.041553	4888.082266	7.324134	-0.038438	3.796661
189.218981	4896.027411	7.329139	-0.038477	3.799616
189.408192	4904.097628	7.334144	-0.038517	3.802615
189.644836	4912.044350	7.339149	-0.038567	3.805567
189.828245	4920.121839	7.344154	-0.038606	3.808564
190.160655	4928.151539	7.349158	-0.038673	3.811545
190.123450	4936.168636	7.354163	-0.038672	3.814510
190.314388	4944.187195	7.359168	-0.038713	3.817478
190.377560	4952.182260	7.364173	-0.038730	3.820433
190.717185	4960.193875	7.369178	-0.038798	3.823397
190.861359	4968.253554	7.374182	-0.038831	3.826373
191.023724	4976.243111	7.379187	-0.038866	3.829321
191.322466	4984.318495	7.384192	-0.038927	3.832301
191.536776	4992.317667	7.389197	-0.038972	3.835249
191.715505	5000.317459	7.394202	-0.039011	3.838194
191.945610	5008.362241	7.399206	-0.039059	3.841154
192.094800	5016.336205	7.404211	-0.039092	3.844084
192.173265	5024.407982	7.409216	-0.039112	3.847047
192.560012	5032.373392	7.414221	-0.039189	3.849974
192.745027	5040.471373	7.419226	-0.039229	3.852944
192.970470	5048.466774	7.424230	-0.039276	3.855874
192.916226	5056.490632	7.429235	-0.039272	3.858808
193.127785	5064.530747	7.434240	-0.039316	3.861750
193.231980	5072.511980	7.439245	-0.039341	3.864666
193.436156	5080.595700	7.444250	-0.039384	3.867619
193.452256	5088.596554	7.449254	-0.039393	3.870537
193.741789	5096.802967	7.454259	-0.039452	3.873532
194.225547	5104.817471	7.459264	-0.039548	3.876459
194.146167	5112.698548	7.464269	-0.039538	3.879324
194.498698	5120.686854	7.469274	-0.039609	3.882234
194.686480	5128.690117	7.474278	-0.039649	3.885144
194.953672	5136.692659	7.479283	-0.039704	3.888054
195.142390	5144.769212	7.484288	-0.039745	3.890986
195.346605	5152.755458	7.489293	-0.039788	3.893884
195.598921	5160.786616	7.494298	-0.039840	3.896797
195.520868	5168.779084	7.499302	-0.039831	3.899687
195.851017	5176.784622	7.504307	-0.039898	3.902588
196.061982	5184.844833	7.509312	-0.039943	3.905504
196.244794	5192.846010	7.514317	-0.039982	3.908396
196.314997	5200.894517	7.519322	-0.040000	3.911301
196.663471	5208.896593	7.524326	-0.040070	3.914192
196.484062	5216.939624	7.529331	-0.040042	3.917085
196.789231	5224.937739	7.534336	-0.040105	3.919970
197.015958	5232.914614	7.539341	-0.040152	3.922843
197.209082	5240.937382	7.544346	-0.040193	3.925730
197.240103	5248.986510	7.549350	-0.040204	3.928621
197.649849	5257.016436	7.554355	-0.040286	3.931510
197.964136	5265.032851	7.559360	-0.040350	3.934391
198.119303	5273.043182	7.564365	-0.040384	3.937264
198.171714	5281.066292	7.569370	-0.040399	3.940138
198.578339	5289.052428	7.574374	-0.040480	3.943002
198.635472	5297.088877	7.579379	-0.040496	3.945877
198.789967	5305.111573	7.584384	-0.040530	3.948746
199.124886	5313.142714	7.589389	-0.040598	3.951619
199.321932	5321.216338	7.594394	-0.040640	3.954503
199.324617	5329.191501	7.599398	-0.040646	3.957346
199.514835	5337.194896	7.604403	-0.040687	3.960200
199.892819	5345.201247	7.609408	-0.040762	3.963057
199.980758	5353.186197	7.614413	-0.040784	3.965899
200.038451	5361.231080	7.619418	-0.040800	3.968760
200.264331	5369.300171	7.624422	-0.040847	3.971630
200.374160	5377.329672	7.629427	-0.040873	3.974482
200.536504	5385.355470	7.634432	-0.040909	3.977331
201.104906	5393.310736	7.639437	-0.041020	3.980160
201.444056	5401.349658	7.644442	-0.041088	3.983013
201.356122	5409.372932	7.649446	-0.041077	3.985851
201.517421	5417.390325	7.654451	-0.041113	3.988690
201.833066	5425.456737	7.659456	-0.041177	3.991546
202.183554	5433.437264	7.664461	-0.041247	3.994370
202.373336	5441.486712	7.669466	-0.041288	3.997214
202.532715	5449.476065	7.674470	-0.041323	4.000034
202.595326	5457.493252	7.679475	-0.041340	4.002860
202.781566	5465.532716	7.684480	-0.041380	4.005694
202.841819	5473.531275	7.689485	-0.041396	4.008510
202.955105	5481.624587	7.694490	-0.041423	4.011358
203.198152	5489.631701	7.699494	-0.041473	4.014176
203.210286	5497.684171	7.704499	-0.041481	4.017003
203.675699	5505.655505	7.709504	-0.041573	4.019808
203.590658	5513.634612	7.714509	-0.041562	4.022605
203.779255	5521.682097	7.719514	-0.041603	4.025428
204.118639	5529.709998	7.724518	-0.041671	4.028244
204.261414	5537.735264	7.729523	-0.041703	4.031054
204.344237	5545.860788	7.734528	-0.041724	4.033897
204.544786	5553.805576	7.739533	-0.041767	4.036676
204.883584	5561.765201	7.744538	-0.041835	4.039461
204.936251	5569.808923	7.749542	-0.041850	4.042268
205.198438	5577.785765	7.754547	-0.041904	4.045054
205.354218	5585.826503	7.759552	-0.041939	4.047858
205.521973	5593.822160	7.764557	-0.041975	4.050645
205.564034	5601.887011	7.769562	-0.041988	4.053452
205.878120	5609.904805	7.774566	-0.042052	4.056244
205.886795	5617.841196	7.779571	-0.042059	4.059002
206.073866	5625.942897	7.784576	-0.042099	4.061818
206.176423	5633.894488	7.789581	-0.042124	4.064579
206.719444	5641.953267	7.794586	-0.042230	4.067381
206.614815	5649.974855	7.799590	-0.042216	4.070160
206.625194	5658.004436	7.804595	-0.042223	4.072940
206.929987	5666.050185	7.809600	-0.042285	4.075729
207.134516	5674.014397	7.814605	-0.042329	4.078486
207.323291	5682.063344	7.819610	-0.042369	4.081270
207.413069	5690.020529	7.824614	-0.042391	4.084019
207.689569	5698.073458	7.829619	-0.042448	4.086802
207.915051	5706.114087	7.834624	-0.042495	4.089578
207.978599	5714.147603	7.839629	-0.042512	4.092348
208.027599	5722.176281	7.844634	-0.042527	4.095114
208.157341	5730.190039	7.849638	-0.042556	4.097874
208.068275	5738.151430	7.854643	-0.042545	4.100611
208.282171	5746.193691	7.859648	-0.042590	4.103378
208.389303	5754.222829	7.864653	-0.042616	4.106137
208.631170	5762.260482	7.869658	-0.042666	4.108899
208.777186	5770.302728	7.874662	-0.042698	4.111659
209.081958	5778.324422	7.879667	-0.042761	4.114413
209.396586	5786.389548	7.884672	-0.042824	4.117180
209.393824	5794.311497	7.889677	-0.042829	4.119892
209.809306	5802.341844	7.894682	-0.042912	4.122644
209.962307	5810.357272	7.899686	-0.042946	4.125386
209.932423	5818.371102	7.904691	-0.042945	4.128123
210.120344	5826.424377	7.909696	-0.042986	4.130875
210.190862	5834.427868	7.914701	-0.043004	4.133607
210.352762	5842.520411	7.919706	-0.043040	4.136368
210.566787	5850.473571	7.924710	-0.043085	4.139080
210.740774	5858.488508	7.929715	-0.043123	4.141811
211.064704	5866.493391	7.934720	-0.043188	4.144539
211.111525	5874.493273	7.939725	-0.043202	4.147260
211.336028	5882.528954	7.944730	-0.043249	4.149993
211.518982	5890.594477	7.949734	-0.043289	4.152734
211.490885	5898.599124	7.954739	-0.043289	4.155450
211.967215	5906.602626	7.959744	-0.043383	4.158170
212.052530	5914.614870	7.964749	-0.043404	4.160887
212.333270	5922.616495	7.969754	-0.043462	4.163600
212.605498	5930.624674	7.974758	-0.043518	4.166314
212.723496	5938.633247	7.979763	-0.043545	4.169024
212.836588	5946.711001	7.984768	-0.043571	4.171756
212.840909	5954.712680	7.989773	-0.043577	4.174459
213.099134	5962.739807	7.994778	-0.043631	4.177171
213.415950	5970.725897	7.999782	-0.043695	4.179869
213.466016	5978.734371	8.004787	-0.043710	4.182570
213.572053	5986.754565	8.009792	-0.043735	4.185273
213.662662	5994.796265	8.014797	-0.043757	4.187982
214.030023	6002.817593	8.019802	-0.043831	4.190685
214.138610	6010.939847	8.024806	-0.043856	4.193417
214.236263	6018.952560	8.029811	-0.043880	4.196111
214.644659	6026.851836	8.034816	-0.043961	4.198768
214.697073	6034.900547	8.039821	-0.043976	4.201469
214.966701	6042.850844	8.044826	-0.044032	4.204139
215.159034	6050.886045	8.049830	-0.044073	4.206834
215.483334	6058.882323	8.054835	-0.044139	4.209516
215.648333	6066.957763	8.059840	-0.044175	4.212221
215.688393	6074.988128	8.064845	-0.044187	4.214908
215.981213	6082.973955	8.069850	-0.044247	4.217580
215.918974	6090.980325	8.074854	-0.044241	4.220255
216.182596	6098.999791	8.079859	-0.044295	4.222935
216.550107	6107.030744	8.084864	-0.044369	4.225618
216.311671	6115.063286	8.089869	-0.044330	4.228294
216.704728	6123.026101	8.094874	-0.044409	4.230952
216.766572	6131.120007	8.099878	-0.044425	4.233648
216.798984	6139.142074	8.104883	-0.044437	4.236318
217.054016	6147.138421	8.109888	-0.044490	4.238980
217.281961	6155.126585	8.114893	-0.044537	4.241638
217.340643	6163.113371	8.119898	-0.044554	4.244292
217.588090	6171.158201	8.124902	-0.044605	4.246965
217.891961	6179.152979	8.129907	-0.044667	4.249620
218.222936	6187.240675	8.134912	-0.044734	4.252304
218.074102	6195.219601	8.139917	-0.044711	4.254947
218.348613	6203.272020	8.144922	-0.044768	4.257616
218.530035	6211.243432	8.149926	-0.044807	4.260256
218.468423	6219.280244	8.154931	-0.044801	4.262913
218.896705	6227.313668	8.159936	-0.044886	4.265572
219.000752	6235.333482	8.164941	-0.044911	4.268222
219.234537	6243.374776	8.169946	-0.044959	4.270878
219.282466	6251.462016	8.174950	-0.044974	4.273547
219.286621	6259.458857	8.179955	-0.044980	4.276183
219.707525	6267.399662	8.184960	-0.045063	4.278803
219.849295	6275.442754	8.189965	-0.045095	4.281453
220.036844	6283.385340	8.194970	-0.045135	4.284068
220.262294	6291.480044	8.199974	-0.045183	4.286732
220.303950	6299.421047	8.204979	-0.045196	4.289343
220.589245	6307.543414	8.209984	-0.045254	4.292013
220.849370	6315.544099	8.214989	-0.045308	4.294641
221.168489	6323.568349	8.219994	-0.045373	4.297276
221.139241	6331.572762	8.224998	-0.045373	4.299900
221.391546	6339.561949	8.230003	-0.045425	4.302520
221.744939	6347.599484	8.235008	-0.045496	4.305155
221.577020	6355.597160	8.240013	-0.045470	4.307771
221.758639	6363.624862	8.245018	-0.045509	4.310397
222.136855	6371.695968	8.250022	-0.045585	4.313038
222.484222	6379.688759	8.255027	-0.045655	4.315652
222.371171	6387.691328	8.260032	-0.045639	4.318263
222.518167	6395.678451	8.265037	-0.045672	4.320870
222.833492	6403.671470	8.270042	-0.045736	4.323479
222.846261	6411.722194	8.275046	-0.045744	4.326102
222.733741	6419.715375	8.280051	-0.045728	4.328704
223.129659	6427.796235	8.285056	-0.045807	4.331337
223.465149	6435.769232	8.290061	-0.045875	4.333933
223.348785	6443.812590	8.295066	-0.045858	4.336546
223.771646	6451.778134	8.300070	-0.045942	4.339137
223.968175	6459.827461	8.305075	-0.045984	4.341752
224.077512	6467.810401	8.310080	-0.046010	4.344343
223.953268	6475.852116	8.315085	-0.045992	4.346950
224.319245	6483.842298	8.320090	-0.046066	4.349541
224.535211	6491.936872	8.325094	-0.046111	4.352165
224.719649	6499.967595	8.330099	-0.046151	4.354765
225.015248	6507.990363	8.335104	-0.046211	4.357362
225.098424	6515.940132	8.340109	-0.046232	4.359933
225.087277	6523.944805	8.345114	-0.046235	4.362519
225.296419	6531.938360	8.350118	-0.046280	4.365102
225.449582	6539.952330	8.355123	-0.046313	4.367689
225.500536	6547.991456	8.360128	-0.046328	4.370282
225.467124	6556.017593	8.365133	-0.046327	4.372869
225.886428	6564.048789	8.370138	-0.046411	4.375459
226.223724	6572.044717	8.375142	-0.046479	4.378035
226.376934	6580.022640	8.380147	-0.046513	4.380603
226.606642	6588.053466	8.385152	-0.046561	4.383187
226.542243	6596.063270	8.390157	-0.046554	4.385760
226.563491	6604.146259	8.395162	-0.046563	4.388357
226.702993	6612.133731	8.400166	-0.046595	4.390921
226.799643	6620.186055	8.405171	-0.046618	4.393505
227.061874	6628.228659	8.410176	-0.046672	4.396085
227.185224	6636.175128	8.415181	-0.046700	4.398632
227.519309	6644.212471	8.420186	-0.046768	4.401208
227.424043	6652.201224	8.425190	-0.046755	4.403764
227.463919	6660.216802	8.430195	-0.046768	4.406328
227.789331	6668.247142	8.435200	-0.046834	4.408897
227.966688	6676.265102	8.440205	-0.046872	4.411459
228.090334	6684.291578	8.445210	-0.046901	4.414023
228.082811	6692.346335	8.450214	-0.046905	4.416593
228.434555	6700.271049	8.455219	-0.046975	4.419122
228.664062	6708.404125	8.460224	-0.047024	4.421716
228.687352	6716.352997	8.465229	-0.047033	4.424248
228.839573	6724.434025	8.470234	-0.047067	4.426822
228.914471	6732.428686	8.475238	-0.047086	4.429366
228.934895	6740.455275	8.480243	-0.047095	4.431918
229.280604	6748.479955	8.485248	-0.047165	4.434470
229.344703	6756.498572	8.490253	-0.047182	4.437017
229.387584	6764.478835	8.495258	-0.047196	4.439551
229.774934	6772.500366	8.500262	-0.047273	4.442098
229.742141	6780.454454	8.505267	-0.047272	4.444620
230.029528	6788.533017	8.510272	-0.047331	4.447181
230.002929	6796.513930	8.515277	-0.047331	4.449708
230.263405	6804.586487	8.520282	-0.047385	4.452265
230.374351	6812.626185	8.525286	-0.047411	4.454808
230.308428	6820.637156	8.530291	-0.047404	4.457341
230.653478	6828.603195	8.535296	-0.047474	4.459860
230.769316	6836.630022	8.540301	-0.047501	4.462395
230.759043	6844.594681	8.545306	-0.047504	4.464909
230.878604	6852.650438	8.550310	-0.047532	4.467450
231.259454	6860.665272	8.555315	-0.047608	4.469979
231.184902	6868.761255	8.560320	-0.047599	4.472529
231.454441	6876.751947	8.565325	-0.047655	4.475047
231.674631	6884.762670	8.570330	-0.047701	4.477569
231.934384	6892.749785	8.575335	-0.047755	4.480082
231.971937	6900.747780	8.580339	-0.047767	4.482596
232.217406	6908.774009	8.585344	-0.047818	4.485119
232.386705	6916.758882	8.590349	-0.047855	4.487627
232.667076	6924.776063	8.595354	-0.047913	4.490144
232.874066	6932.860296	8.600359	-0.047956	4.492680
232.944900	6940.840890	8.605363	-0.047975	4.495182
233.196235	6948.875134	8.610368	-0.048027	4.497700
233.096544	6956.818425	8.615373	-0.048014	4.500187
233.490399	6964.867487	8.620378	-0.048092	4.502707
233.754067	6972.866436	8.625383	-0.048147	4.505209
233.841042	6980.898411	8.630387	-0.048168	4.507720
233.882562	6988.953275	8.635392	-0.048181	4.510237
234.164832	6996.981717	8.640397	-0.048239	4.512745
234.262112	7005.071237	8.645402	-0.048263	4.515269
234.393343	7013.018888	8.650407	-0.048292	4.517749
234.469749	7020.949336	8.655411	-0.048312	4.520221
234.595642	7029.000074	8.660416	-0.048341	4.522730
234.688404	7036.995400	8.665421	-0.048363	4.525219
234.997525	7045.009736	8.670426	-0.048426	4.527714
235.327713	7053.015428	8.675431	-0.048493	4.530205
235.199291	7061.075865	8.680435	-0.048474	4.532710
235.490793	7069.108918	8.685440	-0.048534	4.535207
235.578507	7077.094464	8.690445	-0.048556	4.537686
235.653091	7085.066386	8.695450	-0.048575	4.540161
235.737127	7093.122178	8.700455	-0.048596	4.542659
236.008895	7101.067574	8.705459	-0.048652	4.545123
236.286790	7109.148392	8.710464	-0.048709	4.547627
236.214127	7117.176085	8.715469	-0.048701	4.550113
236.388884	7125.248293	8.720474	-0.048738	4.552611
236.693394	7133.254733	8.725479	-0.048800	4.555088
236.796220	7141.196878	8.730483	-0.048825	4.557544
236.944739	7149.212892	8.735488	-0.048858	4.560021
237.164611	7157.254270	8.740493	-0.048904	4.562504
237.410122	7165.231218	8.745498	-0.048955	4.564967
237.498349	7173.279988	8.750503	-0.048977	4.567450
237.600618	7181.238929	8.755507	-0.049001	4.569904
237.870303	7189.337431	8.760512	-0.049057	4.572399
237.676228	7197.367931	8.765517	-0.049026	4.574872
237.887616	7205.415695	8.770522	-0.049071	4.577350
238.210631	7213.359993	8.775527	-0.049136	4.579794
238.382818	7221.395394	8.780531	-0.049174	4.582265
238.428956	7229.418237	8.785536	-0.049187	4.584730
238.552887	7237.460504	8.790541	-0.049216	4.587200
238.886467	7245.470112	8.795546	-0.049283	4.589659
239.133219	7253.534189	8.800551	-0.049335	4.592133
239.030853	7261.522836	8.805555	-0.049321	4.594583
239.447216	7269.548591	8.810560	-0.049404	4.597043
239.657044	7277.488335	8.815565	-0.049448	4.599475
239.726356	7285.574309	8.820570	-0.049466	4.601950
240.023242	7293.506279	8.825575	-0.049527	4.604377
240.271775	7301.547771	8.830579	-0.049578	4.606836
240.302866	7309.528375	8.835584	-0.049589	4.609276
240.290436	7317.600133	8.840589	-0.049593	4.611741
240.426221	7325.624037	8.845594	-0.049623	4.614191
240.742783	7333.660475	8.850599	-0.049687	4.616643
240.741405	7341.598827	8.855603	-0.049692	4.619065
241.089294	7349.726954	8.860608	-0.049763	4.621542
241.142963	7357.656429	8.865613	-0.049778	4.623958
241.566132	7365.683734	8.870618	-0.049862	4.626402
241.571982	7373.697559	8.875623	-0.049868	4.628841
241.601821	7381.728998	8.880627	-0.049879	4.631284
242.061577	7389.744789	8.885632	-0.049970	4.633721
242.010055	7397.757964	8.890637	-0.049966	4.636156
242.202969	7405.717183	8.895642	-0.050007	4.638573
242.434629	7413.781542	8.900647	-0.050056	4.641020
242.455657	7421.770519	8.905651	-0.050065	4.643444
242.534346	7429.842100	8.910656	-0.050085	4.645891
242.542977	7437.772497	8.915661	-0.050092	4.648295
242.552479	7445.835885	8.920666	-0.050099	4.650737
242.853170	7453.893060	8.925671	-0.050160	4.653176
242.873248	7461.898981	8.930675	-0.050169	4.655598
243.019077	7469.889898	8.935680	-0.050202	4.658015
243.127266	7477.894191	8.940685	-0.050227	4.660434
243.428763	7485.915834	8.945690	-0.050289	4.662857
243.508064	7493.939850	8.950695	-0.050309	4.665280
243.615693	7501.939221	8.955699	-0.050334	4.667693
243.862728	7509.967207	8.960704	-0.050385	4.670115
243.982024	7518.083819	8.965709	-0.050413	4.672561
244.205969	7526.099526	8.970714	-0.050460	4.674976
244.272711	7534.081358	8.975719	-0.050478	4.677380
244.624508	7542.021080	8.980723	-0.050548	4.679769
244.695806	7550.048615	8.985728	-0.050567	4.682184
244.707135	7557.979255	8.990733	-0.050574	4.684569
244.953848	7566.024409	8.995738	-0.050626	4.686986
245.210721	7574.070762	9.000743	-0.050679	4.689402
245.297337	7582.093281	9.005747	-0.050700	4.691811
245.476129	7590.097652	9.010752	-0.050739	4.694212
245.582351	7598.147375	9.015757	-0.050764	4.696626
245.710187	7606.099337	9.020762	-0.050793	4.699009
245.877402	7614.163027	9.025767	-0.050830	4.701425
246.063177	7622.111138	9.030771	-0.050869	4.703804
246.061158	7630.172580	9.035776	-0.050874	4.706217
246.190915	7638.167124	9.040781	-0.050904	4.708608
246.399423	7646.207131	9.045786	-0.050948	4.711012
246.661574	7654.272657	9.050791	-0.051002	4.713421
246.806093	7662.278734	9.055795	-0.051034	4.715812
246.918736	7670.267750	9.060800	-0.051061	4.718197
247.052664	7678.268366	9.065805	-0.051091	4.720583
247.135180	7686.256938	9.070810	-0.051112	4.722965
247.380488	7694.291887	9.075815	-0.051163	4.725360
247.454357	7702.303252	9.080819	-0.051182	4.727746
247.671576	7710.361982	9.085824	-0.051227	4.730145
247.568365	7718.405073	9.090829	-0.051214	4.732539
247.747999	7726.430791	9.095834	-0.051252	4.734926
247.921732	7734.451124	9.100839	-0.051290	4.737310
247.888476	7742.417794	9.105843	-0.051289	4.739677
248.080203	7750.431752	9.110848	-0.051330	4.742057
248.399242	7758.449042	9.115853	-0.051395	4.744436
248.499582	7766.457637	9.120858	-0.051419	4.746812
248.616807	7774.499958	9.125863	-0.051446	4.749196
248.650793	7782.491725	9.130867	-0.051458	4.751565
248.875269	7790.587669	9.135872	-0.051505	4.753963
248.888110	7798.565151	9.140877	-0.051512	4.756325
249.097450	7806.524624	9.145882	-0.051557	4.758680
249.245425	7814.561301	9.150887	-0.051590	4.761056
249.379678	7822.558590	9.155891	-0.051620	4.763420
249.460981	7830.564549	9.160896	-0.051640	4.765786
249.615054	7838.595514	9.165901	-0.051674	4.768157
249.969075	7846.610846	9.170906	-0.051746	4.770522
249.988021	7854.670469	9.175911	-0.051754	4.772900
250.015854	7862.653769	9.180915	-0.051765	4.775255
250.497650	7870.637466	9.185920	-0.051860	4.777606
250.478259	7878.632375	9.190925	-0.051862	4.779962
250.618617	7886.682173	9.195930	-0.051893	4.782332
250.793198	7894.691936	9.200935	-0.051931	4.784688
250.854257	7902.665926	9.205939	-0.051948	4.787034
251.085125	7910.747151	9.210944	-0.051996	4.789409
251.361005	7918.744937	9.215949	-0.052053	4.791758
251.418478	7926.762725	9.220954	-0.052069	4.794113
251.623484	7934.852601	9.225959	-0.052112	4.796488
251.553198	7942.747728	9.230963	-0.052104	4.798805
251.852028	7950.812992	9.235968	-0.052165	4.801169
251.850745	7958.769112	9.240973	-0.052170	4.803502
251.944649	7966.827561	9.245978	-0.052193	4.805862
252.099678	7974.832333	9.250983	-0.052227	4.808206
252.069335	7982.872269	9.255987	-0.052227	4.810560
252.352824	7990.268012	9.260992	-0.052285	4.812722
252.308413	7994.767479	9.265997	-0.052280	4.814039

252.423144	7997.212085	9.271002	-0.052303	4.814753
252.678531	7998.549873	9.276007	-0.052351	4.815143
252.728897	7999.009864	9.281011	-0.052361	4.815277
252.787700	7999.903566	9.286016	-0.052372	4.815538
252.774741	7999.862783	9.291021	-0.052370	4.815526
252.784357	7999.861880	9.296026	-0.052372	4.815526
253.006486	7999.863373	9.301031	-0.052413	4.815525
252.786782	7999.893972	9.306035	-0.052373	4.815535
253.053479	7999.894057	9.311040	-0.052422	4.815534
253.252169	7999.870607	9.316045	-0.052459	4.815526
253.177599	7999.857653	9.321050	-0.052446	4.815523
253.189255	7999.887752	9.326055	-0.052448	4.815532
253.295017	7999.849972	9.331059	-0.052468	4.815520
253.557260	7999.887362	9.336064	-0.052517	4.815530
253.461333	7999.868719	9.341069	-0.052499	4.815525
253.595444	7999.830333	9.346074	-0.052524	4.815513
253.669261	7999.855039	9.351079	-0.052538	4.815520
253.420261	7999.827493	9.356083	-0.052492	4.815513
253.645781	7999.870692	9.361088	-0.052534	4.815524
253.497093	7999.918467	9.366093	-0.052506	4.815539
253.641963	7999.942196	9.371098	-0.052533	4.815545
253.851693	7999.960576	9.376103	-0.052572	4.815550
253.602054	7999.868943	9.381107	-0.052526	4.815524
253.723957	7999.890162	9.386112	-0.052549	4.815530
253.745833	7999.867033	9.391117	-0.052553	4.815523
253.959717	7999.896159	9.396122	-0.052593	4.815530
253.834011	7999.837517	9.401127	-0.052569	4.815514
253.808123	7999.838171	9.406131	-0.052565	4.815514
253.938365	7999.917194	9.411136	-0.052589	4.815537
253.978331	7999.905039	9.416141	-0.052597	4.815533
253.929113	7999.894633	9.421146	-0.052588	4.815530
253.887024	7999.928128	9.426151	-0.052580	4.815540
253.841993	7999.896432	9.431155	-0.052571	4.815531
254.023558	7999.937847	9.436160	-0.052605	4.815542
254.143335	7999.900295	9.441165	-0.052628	4.815531
254.094903	7999.919804	9.446170	-0.052619	4.815537
254.036935	7999.946633	9.451175	-0.052608	4.815545
254.105213	7999.884747	9.456179	-0.052621	4.815526
254.129615	7999.918259	9.461184	-0.052626	4.815536
254.065049	7999.928961	9.466189	-0.052614	4.815539
254.112980	7999.916936	9.471194	-0.052623	4.815536
254.270781	7999.944081	9.476199	-0.052652	4.815543
253.969417	7999.899660	9.481203	-0.052596	4.815531
254.270731	7999.874681	9.486208	-0.052652	4.815523
254.357531	7999.917754	9.491213	-0.052669	4.815535
254.261970	7999.914068	9.496218	-0.052651	4.815534
254.423300	7999.943406	9.501223	-0.052681	4.815542
254.334775	7999.868283	9.506227	-0.052665	4.815520
254.469129	7999.887569	9.511232	-0.052690	4.815525
254.313593	7999.916010	9.516237	-0.052661	4.815534
254.466172	7999.877926	9.521242	-0.052689	4.815523
254.348251	7999.930475	9.526247	-0.052668	4.815538
254.247424	7999.836996	9.531251	-0.052649	4.815512
254.293929	7999.887956	9.536256	-0.052658	4.815526
254.403352	7999.889749	9.541261	-0.052678	4.815526
254.516048	7999.891596	9.546266	-0.052699	4.815526
254.563639	7999.931894	9.551271	-0.052708	4.815538
254.481685	7999.880372	9.556275	-0.052693	4.815523
254.402891	7999.921812	9.561280	-0.052678	4.815536
254.458037	7999.891750	9.566285	-0.052689	4.815527
254.506200	7999.873321	9.571290	-0.052698	4.815521
254.599522	7999.923977	9.576295	-0.052715	4.815535
254.573192	7999.871226	9.581299	-0.052710	4.815520
254.754352	7999.863511	9.586304	-0.052744	4.815517
254.576302	7999.887312	9.591309	-0.052711	4.815525
254.688797	7999.924398	9.596314	-0.052732	4.815535
254.690550	7999.976764	9.601319	-0.052733	4.815550
254.507769	7999.855249	9.606323	-0.052699	4.815516
254.690205	7999.894543	9.611328	-0.052733	4.815526
254.583159	7999.923775	9.616333	-0.052713	4.815535
254.737640	7999.911353	9.621338	-0.052742	4.815531
254.791050	7999.913300	9.626343	-0.052752	4.815531
254.800703	7999.864340	9.631347	-0.052754	4.815517
254.902483	7999.916203	9.636352	-0.052773	4.815532
254.626666	7999.893555	9.641357	-0.052721	4.815526
254.619696	7999.915877	9.646362	-0.052720	4.815533
254.619900	7999.969285	9.651367	-0.052720	4.815548
254.888924	7999.940577	9.656371	-0.052771	4.815539
254.765865	7999.971683	9.661376	-0.052748	4.815548
254.671356	7999.929567	9.666381	-0.052730	4.815537
254.830080	7999.909739	9.671386	-0.052760	4.815530
254.849419	7999.952780	9.676391	-0.052764	4.815542
254.794168	7999.921984	9.681395	-0.052753	4.815534
254.776098	7999.949464	9.686400	-0.052750	4.815542
254.835117	7999.928008	9.691405	-0.052761	4.815535
254.893601	7999.917224	9.696410	-0.052772	4.815532
254.881990	7999.910635	9.701415	-0.052770	4.815530
254.994084	7999.875094	9.706419	-0.052791	4.815519
255.060174	7999.952005	9.711424	-0.052804	4.815541
254.991760	7999.946625	9.716429	-0.052791	4.815540
254.886211	7999.929959	9.721434	-0.052771	4.815536
255.036100	7999.979403	9.726439	-0.052799	4.815549
254.865482	7999.930705	9.731443	-0.052768	4.815536
254.898136	7999.956877	9.736448	-0.052774	4.815543
254.828705	7999.927985	9.741453	-0.052761	4.815535
254.868223	7999.886988	9.746458	-0.052768	4.815523
255.118640	7999.994675	9.751463	-0.052815	4.815553
254.910935	7999.965662	9.756467	-0.052777	4.815546
255.026150	7999.973958	9.761472	-0.052798	4.815548
254.858679	7999.939195	9.766477	-0.052767	4.815538
254.876499	7999.929882	9.771482	-0.052770	4.815536
255.033083	7999.952737	9.776487	-0.052800	4.815542
254.851641	7999.837649	9.781491	-0.052766	4.815509
254.908958	7999.898398	9.786496	-0.052777	4.815526
255.066687	7999.908455	9.791501	-0.052806	4.815528
255.167345	7999.906902	9.796506	-0.052825	4.815528
254.905741	7999.940020	9.801511	-0.052776	4.815538
254.846965	7999.920914	9.806515	-0.052766	4.815533
255.244249	7999.969056	9.811520	-0.052840	4.815545
255.193597	7999.926587	9.816525	-0.052830	4.815533
255.325882	7999.923414	9.821530	-0.052855	4.815532
255.324185	7999.973589	9.826535	-0.052855	4.815546
255.149356	7999.945112	9.831539	-0.052822	4.815539
254.954008	7999.948340	9.836544	-0.052786	4.815541
254.991726	7999.935081	9.841549	-0.052793	4.815537
255.299043	7999.961463	9.846554	-0.052851	4.815543
254.975910	7999.976489	9.851559	-0.052790	4.815549
255.108150	7999.948752	9.856563	-0.052815	4.815540
255.172491	7999.978646	9.861568	-0.052827	4.815548
255.075295	7999.940757	9.866573	-0.052809	4.815538
255.090644	7999.926064	9.871578	-0.052812	4.815533
255.245084	7999.970243	9.876583	-0.052841	4.815546
255.016421	7999.940889	9.881587	-0.052799	4.815538
255.200890	7999.983422	9.886592	-0.052833	4.815550
255.335438	7999.984558	9.891597	-0.052858	4.815549
255.408900	7999.968678	9.896602	-0.052872	4.815544
255.320637	8000.005692	9.901607	-0.052856	4.815556
255.327914	7999.954557	9.906611	-0.052857	4.815541
255.402000	8000.014512	9.911616	-0.052871	4.815558
255.407137	7999.991109	9.916621	-0.052872	4.815551
255.299915	7999.958396	9.921626	-0.052852	4.815542
255.455054	8000.004723	9.926631	-0.052881	4.815555
255.336717	7999.973965	9.931635	-0.052859	4.815546
255.399521	8000.009173	9.936640	-0.052871	4.815556
255.194266	7999.990879	9.941645	-0.052833	4.815552
255.423243	7999.981809	9.946650	-0.052876	4.815548
255.429334	8000.007548	9.951655	-0.052877	4.815556
255.357403	7999.974343	9.956659	-0.052863	4.815546
255.546789	7999.989190	9.961664	-0.052899	4.815550
255.296555	7999.932784	9.966669	-0.052852	4.815534
255.237535	7999.938236	9.971674	-0.052841	4.815536
255.455996	7999.999480	9.976679	-0.052882	4.815553
255.417788	7999.987117	9.981683	-0.052875	4.815550
255.376518	7999.988587	9.986688	-0.052868	4.815550
255.277504	7999.953873	9.991693	-0.052849	4.815541
255.257154	7999.988791	9.996698	-0.052846	4.815551
255.476218	7999.997715	10.001703	-0.052886	4.815552
255.278411	7999.962456	10.006707	-0.052850	4.815543
255.156822	7999.999994	10.011712	-0.052827	4.815555
255.085190	7999.956114	10.016717	-0.052814	4.815542
254.998971	7999.940832	10.021722	-0.052798	4.815538
255.223592	7999.971205	10.026727	-0.052840	4.815546
255.363387	7999.947864	10.031731	-0.052866	4.815538
255.354145	7999.997916	10.036736	-0.052864	4.815553
255.522394	7999.981447	10.041741	-0.052896	4.815547
255.433738	7999.921270	10.046746	-0.052879	4.815530
255.459353	7999.997521	10.051751	-0.052884	4.815552
255.290793	7999.944584	10.056755	-0.052853	4.815538
255.525130	8000.006087	10.061760	-0.052897	4.815555
255.599141	7999.990216	10.066765	-0.052911	4.815550
255.478173	7999.970094	10.071770	-0.052888	4.815544
255.451394	8000.000636	10.076775	-0.052883	4.815553
255.242948	7999.966271	10.081779	-0.052844	4.815544
255.268667	7999.960291	10.086784	-0.052849	4.815542
255.402295	7999.969956	10.091789	-0.052874	4.815545
255.351606	7999.975545	10.096794	-0.052865	4.815547
255.321703	7999.993220	10.101799	-0.052860	4.815552
255.213324	7999.954081	10.106803	-0.052839	4.815541
255.333521	7999.976342	10.111808	-0.052862	4.815547
255.439788	7999.943910	10.116813	-0.052882	4.815537
255.465567	7999.935795	10.121818	-0.052887	4.815534
255.438306	7999.999436	10.126823	-0.052882	4.815553
255.478187	7999.974464	10.131827	-0.052889	4.815546
255.490542	7999.976810	10.136832	-0.052892	4.815546
255.299438	7999.995058	10.141837	-0.052856	4.815552
255.397322	7999.977440	10.146842	-0.052874	4.815547
255.593381	7999.994533	10.151847	-0.052911	4.815551
255.414444	7999.935018	10.156851	-0.052878	4.815534
255.501142	7999.954596	10.161856	-0.052894	4.815540
255.409720	7999.950976	10.166861	-0.052877	4.815539
255.300163	7999.971623	10.171866	-0.052857	4.815546
255.403485	7999.979726	10.176871	-0.052876	4.815547
255.592508	7999.933693	10.181875	-0.052911	4.815533
255.654350	8000.004129	10.186880	-0.052923	4.815553
255.558325	7999.968394	10.191885	-0.052905	4.815543
255.565045	7999.971716	10.196890	-0.052907	4.815544
255.783798	8000.024422	10.201895	-0.052947	4.815559
255.603146	7999.975558	10.206899	-0.052914	4.815545
255.679542	8000.034484	10.211904	-0.052928	4.815562
255.662437	8000.010718	10.216909	-0.052925	4.815555
255.527970	8000.014938	10.221914	-0.052900	4.815557
255.503762	8000.029503	10.226919	-0.052896	4.815562
255.615407	8000.002499	10.231923	-0.052917	4.815553
255.738785	7999.999181	10.236928	-0.052940	4.815552
255.492675	7999.984492	10.241933	-0.052894	4.815548
255.553143	7999.998303	10.246938	-0.052905	4.815552
255.607870	7999.983185	10.251943	-0.052916	4.815547
255.361528	7999.982375	10.256947	-0.052870	4.815548
255.624246	7999.988808	10.261952	-0.052919	4.815549
255.417244	7999.975825	10.266957	-0.052880	4.815546
255.475205	7999.987459	10.271962	-0.052891	4.815549
255.561177	7999.997415	10.276967	-0.052907	4.815552
255.649492	7999.944398	10.281971	-0.052924	4.815536
255.652873	7999.988248	10.286976	-0.052925	4.815549
255.611210	7999.952333	10.291981	-0.052917	4.815538
255.518786	7999.958308	10.296986	-0.052900	4.815541
255.870780	7999.997170	10.301991	-0.052965	4.815550
255.789803	7999.980905	10.306995	-0.052950	4.815546
255.538196	8000.009912	10.312000	-0.052904	4.815556
255.727904	7999.977774	10.317005	-0.052939	4.815545
255.792095	7999.975627	10.322010	-0.052951	4.815544
255.774983	8000.021278	10.327015	-0.052948	4.815558
255.755390	7999.989995	10.332019	-0.052945	4.815549
255.837339	8000.034061	10.337024	-0.052960	4.815561
255.607198	7999.985456	10.342029	-0.052917	4.815548
255.630219	7999.942054	10.347034	-0.052921	4.815535
255.807076	8000.011163	10.352039	-0.052955	4.815555
255.557294	7999.967579	10.357043	-0.052908	4.815543
255.496976	8000.014661	10.362048	-0.052897	4.815557
255.587551	7999.989448	10.367053	-0.052914	4.815549
255.778030	7999.984022	10.372058	-0.052950	4.815547
255.769511	8000.007387	10.377063	-0.052948	4.815554
255.509336	7999.924118	10.382067	-0.052900	4.815531
255.722996	7999.987420	10.387072	-0.052940	4.815548
255.818889	7999.992198	10.392077	-0.052957	4.815549
255.806040	7999.980249	10.397082	-0.052955	4.815546
255.849079	8000.018339	10.402087	-0.052963	4.815557
255.732733	7999.957709	10.407091	-0.052942	4.815539
255.661543	7999.974710	10.412096	-0.052929	4.815545
255.555766	8000.000759	10.417101	-0.052909	4.815553
255.594258	8000.005667	10.422106	-0.052916	4.815554
255.710597	8000.037478	10.427111	-0.052938	4.815563
255.512879	8000.006491	10.432115	-0.052901	4.815555
255.798090	7999.986592	10.437120	-0.052954	4.815547
255.764118	7999.976434	10.442125	-0.052948	4.815545
255.620344	7999.952735	10.447130	-0.052922	4.815538
255.902647	7999.970168	10.452135	-0.052974	4.815542
255.883158	7999.961314	10.457139	-0.052971	4.815540
255.720332	8000.014199	10.462144	-0.052940	4.815556
255.915032	8000.007774	10.467149	-0.052977	4.815553
255.804326	7999.982479	10.472154	-0.052956	4.815546
255.811636	7999.981538	10.477159	-0.052958	4.815546
255.711259	7999.954276	10.482163	-0.052939	4.815538
255.710569	7999.971361	10.487168	-0.052939	4.815543
255.575795	7999.936062	10.492173	-0.052914	4.815534
255.671004	7999.926944	10.497178	-0.052932	4.815531
255.921395	8000.019683	10.502183	-0.052979	4.815557
255.695453	7999.976487	10.507187	-0.052937	4.815545
255.542124	7999.965448	10.512192	-0.052908	4.815542
255.620496	7999.961396	10.517197	-0.052923	4.815541
255.666668	7999.965361	10.522202	-0.052932	4.815542
255.731533	7999.987788	10.527207	-0.052944	4.815548
255.625920	7999.959373	10.532211	-0.052924	4.815540
255.873984	8000.013626	10.537216	-0.052970	4.815555
255.863230	8000.016662	10.542221	-0.052969	4.815556
255.849587	8000.014312	10.547226	-0.052966	4.815555
255.782438	8000.021767	10.552231	-0.052954	4.815558
255.759776	7999.991502	10.557235	-0.052950	4.815549
255.703290	8000.006608	10.562240	-0.052939	4.815554
255.738051	8000.014659	10.567245	-0.052946	4.815556
255.814671	7999.987083	10.572250	-0.052960	4.815547
255.807484	8000.011537	10.577255	-0.052959	4.815555
255.803152	7999.976231	10.582259	-0.052958	4.815544
255.855922	8000.011276	10.587264	-0.052968	4.815554
255.661019	8000.007035	10.592269	-0.052932	4.815554
255.921720	8000.005959	10.597274	-0.052980	4.815552
255.823522	8000.059899	10.602279	-0.052962	4.815569
255.963212	8000.014129	10.607283	-0.052988	4.815555
255.886603	8000.052402	10.612288	-0.052974	4.815566
256.000280	8000.021158	10.617293	-0.052995	4.815557
256.059506	8000.015726	10.622298	-0.053007	4.815555
255.970180	8000.012139	10.627303	-0.052990	4.815554
255.986218	8000.017749	10.632307	-0.052993	4.815556
256.100932	8000.042058	10.637312	-0.053015	4.815562
255.984324	8000.018803	10.642317	-0.052993	4.815556
255.747050	8000.009597	10.647322	-0.052949	4.815554
255.951451	8000.016146	10.652327	-0.052987	4.815555
255.831557	8000.010993	10.657331	-0.052965	4.815554
255.974279	8000.034691	10.662336	-0.052991	4.815561
256.013767	8000.024664	10.667341	-0.052999	4.815557
255.909052	8000.009079	10.672346	-0.052980	4.815553
255.894504	8000.040889	10.677351	-0.052977	4.815563
255.808048	7999.980746	10.682355	-0.052961	4.815546
256.081212	7999.989486	10.687360	-0.053012	4.815547
255.921840	7999.998640	10.692365	-0.052982	4.815550
255.964190	7999.964096	10.697370	-0.052990	4.815540
256.027600	8000.028151	10.702375	-0.053002	4.815558
255.994706	7999.994515	10.707379	-0.052996	4.815549
255.987141	8000.037119	10.712384	-0.052995	4.815561
256.070579	8000.007518	10.717389	-0.053010	4.815552
256.071135	8000.042778	10.722394	-0.053011	4.815562
256.084808	8000.043010	10.727399	-0.053013	4.815562
255.844745	7999.969679	10.732403	-0.052969	4.815542
255.974193	7999.991025	10.737408	-0.052993	4.815548
256.035993	8000.005926	10.742413	-0.053004	4.815552
255.761209	7999.972612	10.747418	-0.052953	4.815543
255.928631	8000.035161	10.752423	-0.052985	4.815561
255.877942	7999.988418	10.757427	-0.052975	4.815547
256.020869	7999.945904	10.762432	-0.053002	4.815534
255.987848	7999.993432	10.767437	-0.052996	4.815548
256.023279	7999.982271	10.772442	-0.053003	4.815545
256.030527	8000.014437	10.777447	-0.053004	4.815554
256.036778	8000.009208	10.782451	-0.053005	4.815553
256.144239	8000.024854	10.787456	-0.053025	4.815557
256.187952	8000.012761	10.792461	-0.053034	4.815553
255.940211	8000.015131	10.797466	-0.052988	4.815555
256.077020	8000.036597	10.802471	-0.053013	4.815561
256.054088	8000.023415	10.807475	-0.053009	4.815557
256.182997	8000.026596	10.812480	-0.053033	4.815557
255.882371	7999.988588	10.817485	-0.052977	4.815547
255.999443	7999.968080	10.822490	-0.052999	4.815541
255.991911	8000.008549	10.827495	-0.052998	4.815553
255.926548	8000.022441	10.832499	-0.052986	4.815557
256.141708	8000.023827	10.837504	-0.053026	4.815557
256.131823	8000.018334	10.842509	-0.053024	4.815555
255.948951	7999.929917	10.847514	-0.052990	4.815530
256.160197	8000.001725	10.852519	-0.053030	4.815550
256.033440	7999.974032	10.857523	-0.053006	4.815542
256.013397	7999.988665	10.862528	-0.053002	4.815547
255.829292	8000.005959	10.867533	-0.052968	4.815553
255.970865	8000.021094	10.872538	-0.052995	4.815557
256.063787	8000.029028	10.877543	-0.053012	4.815558
256.004486	7999.980008	10.882547	-0.053001	4.815544
256.070530	8000.017406	10.887552	-0.053014	4.815555
256.150387	8000.008038	10.892557	-0.053029	4.815552
256.091252	8000.016693	10.897562	-0.053018	4.815555
255.942482	8000.028156	10.902567	-0.052990	4.815559
255.969066	8000.014714	10.907571	-0.052995	4.815555
256.166330	8000.039303	10.912576	-0.053032	4.815561
256.027679	8000.018891	10.917581	-0.053006	4.815556
255.866671	7999.993843	10.922586	-0.052976	4.815549
255.962247	8000.029587	10.927591	-0.052994	4.815559
255.929300	8000.010902	10.932595	-0.052988	4.815554
255.893828	8000.032758	10.937600	-0.052982	4.815560
255.937002	8000.017452	10.942605	-0.052990	4.815556
255.979824	7999.982915	10.947610	-0.052998	4.815545
256.079449	8000.044358	10.952615	-0.053016	4.815563
255.975565	8000.015970	10.957619	-0.052997	4.815555
256.097887	8000.037199	10.962624	-0.053020	4.815561
256.093204	8000.012567	10.967629	-0.053019	4.815553
256.173214	7999.996794	10.972634	-0.053034	4.815548
256.145309	8000.019842	10.977639	-0.053029	4.815555
255.979140	7999.964806	10.982643	-0.052998	4.815540
255.993749	8000.034471	10.987648	-0.053001	4.815560
256.201155	8000.028254	10.992653	-0.053040	4.815557
256.111167	8000.034269	10.997658	-0.053023	4.815560
255.882582	8000.057244	11.002663	-0.052981	4.815567
255.940131	8000.036832	11.007667	-0.052992	4.815561
256.170362	8000.013900	11.012672	-0.053034	4.815553
256.051662	8000.011970	11.017677	-0.053012	4.815553
256.306334	8000.019341	11.022682	-0.053060	4.815554
256.406105	8000.046611	11.027687	-0.053079	4.815562
256.317752	7999.989640	11.032691	-0.053062	4.815546
256.262741	8000.040014	11.037696	-0.053052	4.815561
256.313635	8000.034445	11.042701	-0.053062	4.815559
256.305059	8000.043925	11.047706	-0.053060	4.815562
256.277614	8000.062709	11.052711	-0.053055	4.815567
256.087311	8000.024365	11.057715	-0.053020	4.815557
256.311970	8000.066490	11.062720	-0.053062	4.815568
256.176792	8000.049339	11.067725	-0.053037	4.815564
256.159664	8000.031979	11.072730	-0.053034	4.815559
256.374394	8000.058990	11.077735	-0.053074	4.815566
256.341882	8000.006136	11.082739	-0.053068	4.815550
256.071375	8000.023086	11.087744	-0.053017	4.815557
256.226118	8000.018145	11.092749	-0.053046	4.815554
256.171406	8000.050368	11.097754	-0.053036	4.815564
256.338334	8000.066986	11.102759	-0.053067	4.815568
256.134610	8000.030559	11.107763	-0.053030	4.815558
256.419809	8000.058721	11.112768	-0.053083	4.815565
256.392450	8000.045466	11.117773	-0.053078	4.815562
256.091873	8000.016002	11.122778	-0.053022	4.815554
256.321000	8000.053928	11.127783	-0.053065	4.815564
256.266183	7999.996437	11.132787	-0.053055	4.815548
256.297625	8000.009775	11.137792	-0.053061	4.815552
256.411762	8000.019123	11.142797	-0.053082	4.815554
256.436337	8000.018464	11.147802	-0.053087	4.815553
256.369320	8000.055826	11.152807	-0.053074	4.815565
256.390750	8000.017736	11.157811	-0.053078	4.815553
256.636684	8000.036713	11.162816	-0.053124	4.815558
256.489505	8000.012957	11.167821	-0.053097	4.815552
256.352396	8000.008590	11.172826	-0.053071	4.815551
256.315887	8000.034702	11.177831	-0.053065	4.815559
256.061918	8000.004931	11.182835	-0.053017	4.815551
256.154522	8000.036355	11.187840	-0.053035	4.815560
256.101022	8000.044034	11.192845	-0.053025	4.815562
256.248227	8000.036834	11.197850	-0.053052	4.815560
256.323830	8000.060504	11.202855	-0.053067	4.815566
256.239084	8000.013205	11.207859	-0.053051	4.815553
256.320442	8000.054058	11.212864	-0.053066	4.815564
256.358968	8000.034403	11.217869	-0.053073	4.815558
256.213851	8000.027769	11.222874	-0.053047	4.815557
256.378317	8000.066775	11.227879	-0.053077	4.815568
256.500886	8000.017521	11.232883	-0.053100	4.815553
256.262511	8000.053152	11.237888	-0.053056	4.815564
256.303129	8000.042076	11.242893	-0.053064	4.815561
256.472026	8000.005326	11.247898	-0.053095	4.815549
256.310764	8000.037945	11.252903	-0.053065	4.815560
256.354637	8000.009834	11.257907	-0.053073	4.815551
256.418548	8000.035449	11.262912	-0.053085	4.815558
256.528947	8000.020173	11.267917	-0.053106	4.815553
256.365537	8000.030328	11.272922	-0.053076	4.815557
256.273060	8000.021350	11.277927	-0.053059	4.815555
256.398807	8000.022344	11.282931	-0.053082	4.815555
256.325457	8000.042514	11.287936	-0.053069	4.815561
256.254825	8000.034961	11.292941	-0.053055	4.815559
256.353514	8000.041920	11.297946	-0.053074	4.815561
256.418675	8000.039789	11.302951	-0.053086	4.815560
256.279474	8000.011892	11.307955	-0.053060	4.815552
256.339141	8000.059866	11.312960	-0.053072	4.815566
256.541689	8000.034346	11.317965	-0.053109	4.815557
256.327022	7999.965701	11.322970	-0.053069	4.815538
256.397423	8000.038414	11.327975	-0.053083	4.815559
256.488518	8000.006802	11.332979	-0.053100	4.815550
256.527056	8000.036276	11.337984	-0.053107	4.815558
256.495060	8000.000518	11.342989	-0.053101	4.815548
256.596368	7999.977616	11.347994	-0.053120	4.815541
256.538337	8000.022601	11.352999	-0.053109	4.815554
256.297373	7999.989838	11.358003	-0.053065	4.815546
256.378304	8000.040295	11.363008	-0.053080	4.815560
256.657616	8000.021369	11.368013	-0.053132	4.815553
256.334682	8000.017171	11.373018	-0.053072	4.815553
256.491607	8000.054986	11.378023	-0.053101	4.815564
256.509654	8000.025385	11.383027	-0.053105	4.815555
256.309580	8000.046690	11.388032	-0.053067	4.815562
256.245811	8000.016821	11.393037	-0.053056	4.815554
256.458733	7999.998946	11.398042	-0.053095	4.815547
256.541711	8000.040894	11.403047	-0.053111	4.815559
256.271841	8000.010862	11.408051	-0.053061	4.815552
256.457249	8000.047006	11.413056	-0.053095	4.815562
256.591195	8000.048134	11.418061	-0.053120	4.815561
256.566673	8000.017838	11.423066	-0.053116	4.815552
256.400269	8000.052508	11.428071	-0.053085	4.815563
256.299495	8000.033783	11.433075	-0.053066	4.815558
256.338672	8000.022683	11.438080	-0.053074	4.815555
256.523732	8000.038529	11.443085	-0.053108	4.815559
256.321109	8000.024548	11.448090	-0.053071	4.815556
256.489642	8000.054009	11.453095	-0.053102	4.815563
256.415847	8000.021840	11.458099	-0.053088	4.815554
256.291422	8000.039040	11.463104	-0.053065	4.815560
256.431023	8000.033852	11.468109	-0.053092	4.815558
256.510225	8000.016997	11.473114	-0.053106	4.815552
256.428287	8000.043435	11.478119	-0.053091	4.815561
256.556829	8000.024183	11.483123	-0.053115	4.815554
256.695842	8000.029666	11.488128	-0.053141	4.815555
256.409823	8000.025002	11.493133	-0.053088	4.815555
256.452200	8000.027839	11.498138	-0.053096	4.815556
256.646381	8000.065195	11.503143	-0.053132	4.815566
256.381704	8000.033112	11.508147	-0.053083	4.815558
256.375610	8000.044768	11.513152	-0.053082	4.815561
256.587068	8000.025802	11.518157	-0.053121	4.815555
256.545975	8000.014459	11.523162	-0.053114	4.815552
256.669353	8000.033570	11.528167	-0.053137	4.815557
256.500467	7999.983828	11.533171	-0.053106	4.815543
256.639787	8000.051260	11.538176	-0.053132	4.815562
256.607735	8000.053949	11.543181	-0.053126	4.815563
256.575118	8000.038472	11.548186	-0.053120	4.815558
256.680888	8000.058364	11.553191	-0.053140	4.815564
256.474425	8000.033640	11.558195	-0.053101	4.815557
256.341687	8000.060316	11.563200	-0.053077	4.815566
256.548139	8000.027384	11.568205	-0.053115	4.815555
256.486986	7999.998625	11.573210	-0.053104	4.815547
256.607508	8000.040118	11.578215	-0.053126	4.815559
256.329786	8000.052678	11.583219	-0.053075	4.815564
256.441790	8000.027816	11.588224	-0.053096	4.815556
256.641618	8000.023611	11.593229	-0.053133	4.815554
256.628892	8000.006324	11.598234	-0.053131	4.815549
256.471054	8000.041134	11.603239	-0.053101	4.815560
256.548946	8000.024258	11.608243	-0.053116	4.815554
256.539285	8000.044401	11.613248	-0.053114	4.815560
256.566199	8000.034168	11.618253	-0.053119	4.815557
256.487378	8000.015801	11.623258	-0.053105	4.815552
256.544882	8000.068013	11.628263	-0.053116	4.815567
256.455964	8000.030256	11.633267	-0.053099	4.815557
256.437714	8000.034239	11.638272	-0.053096	4.815558
256.569542	8000.026788	11.643277	-0.053121	4.815555
256.353951	8000.012595	11.648282	-0.053080	4.815552
256.539992	8000.055158	11.653287	-0.053115	4.815563
256.507262	8000.019387	11.658291	-0.053109	4.815553
256.434804	8000.032096	11.663296	-0.053096	4.815557
256.389017	8000.036696	11.668301	-0.053087	4.815559
256.478735	8000.024286	11.673306	-0.053104	4.815555
256.430310	8000.019231	11.678311	-0.053095	4.815553
256.350790	8000.036096	11.683315	-0.053081	4.815559
256.392433	8000.031445	11.688320	-0.053088	4.815557
256.467006	8000.027331	11.693325	-0.053102	4.815556
256.486132	8000.026583	11.698330	-0.053106	4.815555
256.477874	8000.042477	11.703335	-0.053105	4.815560
256.569666	8000.029032	11.708339	-0.053122	4.815556
256.632158	8000.048217	11.713344	-0.053134	4.815561
256.485319	8000.046895	11.718349	-0.053106	4.815561
256.593226	8000.032645	11.723354	-0.053126	4.815557
256.570994	8000.058990	11.728359	-0.053122	4.815564
256.361335	8000.019262	11.733363	-0.053083	4.815554
256.514101	8000.017493	11.738368	-0.053112	4.815552
256.437144	7999.983137	11.743373	-0.053098	4.815543
256.434702	7999.999125	11.748378	-0.053097	4.815547
256.517134	8000.054947	11.753383	-0.053113	4.815563
256.452419	8000.033607	11.758387	-0.053101	4.815557
256.364160	8000.077029	11.763392	-0.053085	4.815571
256.379049	8000.059125	11.768397	-0.053087	4.815565
256.587761	8000.046522	11.773402	-0.053126	4.815561
256.568287	8000.063300	11.778407	-0.053123	4.815566
256.475758	8000.024417	11.783411	-0.053106	4.815555
256.560364	8000.072799	11.788416	-0.053122	4.815568
256.724478	8000.077624	11.793421	-0.053152	4.815569
256.752035	8000.033226	11.798426	-0.053157	4.815556
256.521388	8000.031603	11.803431	-0.053115	4.815557
256.506271	7999.986508	11.808435	-0.053112	4.815543
256.739241	8000.011681	11.813440	-0.053155	4.815550
256.673208	8000.022359	11.818445	-0.053143	4.815553
256.522320	8000.002814	11.823450	-0.053115	4.815548
256.591848	8000.032794	11.828455	-0.053128	4.815557
256.446745	8000.006936	11.833459	-0.053101	4.815550
256.306014	8000.004646	11.838464	-0.053075	4.815550
256.640377	8000.020795	11.843469	-0.053137	4.815553
256.582506	7999.997430	11.848474	-0.053127	4.815546
256.641518	8000.015490	11.853479	-0.053138	4.815551
256.669973	7999.983923	11.858483	-0.053143	4.815542
256.659852	8000.030758	11.863488	-0.053141	4.815556
256.584729	8000.026335	11.868493	-0.053128	4.815555
256.535057	7999.988152	11.873498	-0.053118	4.815544
256.716955	8000.031715	11.878503	-0.053152	4.815556
256.456811	8000.037086	11.883507	-0.053104	4.815558
256.354600	8000.017269	11.888512	-0.053085	4.815553
256.893426	8000.030350	11.893517	-0.053186	4.815554
256.765209	7999.985544	11.898522	-0.053162	4.815542
256.720920	8000.071337	11.903527	-0.053154	4.815567
256.851067	8000.035023	11.908531	-0.053178	4.815556
256.640039	8000.034788	11.913536	-0.053139	4.815557
256.602549	8000.041660	11.918541	-0.053132	4.815559
256.740533	8000.019358	11.923546	-0.053158	4.815552
256.869622	8000.046039	11.928551	-0.053182	4.815559
256.701676	8000.027283	11.933555	-0.053151	4.815554
256.665844	8000.032046	11.938560	-0.053144	4.815556
256.822678	8000.013256	11.943565	-0.053173	4.815550
256.744662	8000.004514	11.948570	-0.053159	4.815547
256.603074	8000.015026	11.953575	-0.053133	4.815551
256.610100	7999.998060	11.958579	-0.053134	4.815546
256.751389	8000.042029	11.963584	-0.053160	4.815558
256.701497	8000.029474	11.968589	-0.053151	4.815555
256.734585	7999.991574	11.973594	-0.053157	4.815544
256.847200	8000.024394	11.978599	-0.053178	4.815553
256.692374	7999.969541	11.983603	-0.053150	4.815537
256.582204	8000.023286	11.988608	-0.053129	4.815554
256.614409	8000.028092	11.993613	-0.053135	4.815555
256.608943	8000.002379	11.998618	-0.053134	4.815547
256.626508	8000.058210	12.003623	-0.053138	4.815564
256.584007	7999.999852	12.008627	-0.053130	4.815547
256.573526	8000.007165	12.013632	-0.053128	4.815549
256.599036	8000.046038	12.018637	-0.053133	4.815560
256.530335	8000.018224	12.023642	-0.053120	4.815552
256.672271	8000.064339	12.028647	-0.053147	4.815565
256.616519	8000.034600	12.033651	-0.053137	4.815557
256.537990	8000.030121	12.038656	-0.053122	4.815556
256.812879	8000.025007	12.043661	-0.053173	4.815553
256.693546	7999.994230	12.048666	-0.053151	4.815545
256.710819	8000.036173	12.053671	-0.053154	4.815557
256.719297	7999.993599	12.058675	-0.053156	4.815544
256.748861	8000.042151	12.063680	-0.053162	4.815558
256.668064	8000.056859	12.068685	-0.053147	4.815563
256.693690	8000.025246	12.073690	-0.053152	4.815554
256.775149	8000.044740	12.078695	-0.053167	4.815559
256.570310	8000.012567	12.083699	-0.053129	4.815551
256.635972	8000.031803	12.088704	-0.053141	4.815556
256.636737	8000.022212	12.093709	-0.053141	4.815553
256.617746	8000.020842	12.098714	-0.053138	4.815553
256.740402	8000.036738	12.103719	-0.053161	4.815557
256.734711	8000.030245	12.108723	-0.053160	4.815555
256.710956	8000.020253	12.113728	-0.053156	4.815552
256.667767	8000.031304	12.118733	-0.053148	4.815556
256.665467	8000.014186	12.123738	-0.053147	4.815551
256.633486	8000.048916	12.128743	-0.053141	4.815561
256.653413	8000.021482	12.133747	-0.053145	4.815553
256.672628	8000.032484	12.138752	-0.053149	4.815556
256.895711	8000.038272	12.143757	-0.053191	4.815557
256.681355	8000.037983	12.148762	-0.053151	4.815557
256.680174	8000.045448	12.153767	-0.053151	4.815560
256.721466	8000.029042	12.158771	-0.053158	4.815555
256.816974	8000.024202	12.163776	-0.053176	4.815553
256.564805	8000.033976	12.168781	-0.053129	4.815557
256.501111	7999.982747	12.173786	-0.053118	4.815542
256.775375	8000.013935	12.178791	-0.053169	4.815550
256.868862	8000.010130	12.183795	-0.053186	4.815548
256.653365	8000.036523	12.188800	-0.053146	4.815557
256.622985	8000.032831	12.193805	-0.053141	4.815556
256.641093	8000.023523	12.198810	-0.053144	4.815553
256.652430	8000.032260	12.203815	-0.053146	4.815556
256.532641	7999.989727	12.208819	-0.053124	4.815544
256.721118	8000.024854	12.213824	-0.053159	4.815553
256.730570	8000.041037	12.218829	-0.053161	4.815558
256.723581	8000.031319	12.223834	-0.053160	4.815555
256.815575	8000.064870	12.228839	-0.053177	4.815565
256.879526	8000.033882	12.233843	-0.053189	4.815555
256.822846	8000.052189	12.238848	-0.053179	4.815561
256.887352	8000.050047	12.243853	-0.053191	4.815560
256.476437	8000.055091	12.248858	-0.053114	4.815563
256.609901	8000.066891	12.253863	-0.053139	4.815566
256.467283	8000.034666	12.258867	-0.053113	4.815557
256.751607	8000.051066	12.263872	-0.053166	4.815561
256.812770	8000.053141	12.268877	-0.053177	4.815561
256.426447	8000.030819	12.273882	-0.053106	4.815557
256.800424	8000.076452	12.278887	-0.053175	4.815568
256.916485	8000.037772	12.283891	-0.053197	4.815556
256.948223	8000.048979	12.288896	-0.053203	4.815559
256.928326	8000.051866	12.293901	-0.053199	4.815560
256.738060	8000.032746	12.298906	-0.053164	4.815556
256.742444	8000.052050	12.303911	-0.053165	4.815561
256.555187	8000.011619	12.308915	-0.053130	4.815550
256.779430	8000.030242	12.313920	-0.053172	4.815555
256.893051	8000.015018	12.318925	-0.053193	4.815550
256.881212	7999.991336	12.323930	-0.053191	4.815543
257.045307	8000.023930	12.328935	-0.053222	4.815552
256.862612	8000.034837	12.333939	-0.053188	4.815556
256.740716	8000.055283	12.338944	-0.053165	4.815562
256.690244	8000.051262	12.343949	-0.053156	4.815561
256.853849	8000.036855	12.348954	-0.053187	4.815556
256.931173	8000.047738	12.353959	-0.053201	4.815559
256.757560	8000.038502	12.358963	-0.053169	4.815557
256.782767	8000.044262	12.363968	-0.053174	4.815559
257.016130	8000.047015	12.368973	-0.053217	4.815558
256.802160	8000.011487	12.373978	-0.053177	4.815549
257.143772	8000.052320	12.378983	-0.053241	4.815559
256.927231	8000.017818	12.383987	-0.053201	4.815550
256.864080	8000.028543	12.388992	-0.053189	4.815554
256.844018	8000.026088	12.393997	-0.053186	4.815553
256.821450	8000.006503	12.399002	-0.053181	4.815547
256.886749	8000.047094	12.404007	-0.053194	4.815559
256.648794	8000.030399	12.409011	-0.053150	4.815555
256.736529	8000.015820	12.414016	-0.053166	4.815551
256.829529	7999.993851	12.419021	-0.053183	4.815544
256.737707	7999.977408	12.424026	-0.053166	4.815539
256.847500	8000.030474	12.429031	-0.053187	4.815554
256.828236	8000.017351	12.434035	-0.053183	4.815551
256.862114	8000.038205	12.439040	-0.053190	4.815557
256.973587	8000.045374	12.444045	-0.053211	4.815558
256.943088	8000.023524	12.449050	-0.053205	4.815552
256.971214	8000.041080	12.454055	-0.053210	4.815557
256.901813	7999.996165	12.459059	-0.053198	4.815544
256.984117	7999.976158	12.464064	-0.053213	4.815538
256.763302	8000.054796	12.469069	-0.053172	4.815562
256.766800	8000.058065	12.474074	-0.053173	4.815563
256.772711	8000.082734	12.479079	-0.053174	4.815570
256.759165	8000.052617	12.484083	-0.053172	4.815561
256.641610	8000.060317	12.489088	-0.053150	4.815564
256.673928	8000.062989	12.494093	-0.053156	4.815565
256.984990	8000.022154	12.499098	-0.053214	4.815551
256.940001	8000.038515	12.504103	-0.053206	4.815556
256.672619	8000.045904	12.509107	-0.053156	4.815560
256.886892	8000.061160	12.514112	-0.053196	4.815563
257.136711	8000.033209	12.519117	-0.053242	4.815554
256.823443	8000.021692	12.524122	-0.053184	4.815552
256.771969	8000.072124	12.529127	-0.053175	4.815567
256.986578	8000.036121	12.534131	-0.053215	4.815555
257.065264	8000.061979	12.539136	-0.053230	4.815562
257.017760	8000.070823	12.544141	-0.053221	4.815565
256.816368	8000.041909	12.549146	-0.053183	4.815558
256.824569	8000.048459	12.554151	-0.053185	4.815560
256.820151	8000.030239	12.559155	-0.053184	4.815554
256.559528	8000.030262	12.564160	-0.053136	4.815556
256.788913	8000.054309	12.569165	-0.053179	4.815562
256.788514	8000.047903	12.574170	-0.053179	4.815560
256.699365	8000.046455	12.579175	-0.053162	4.815560
256.901033	8000.025193	12.584179	-0.053200	4.815552
256.887970	8000.036736	12.589184	-0.053197	4.815556
257.003792	8000.043976	12.594189	-0.053219	4.815557
256.903089	8000.004959	12.599194	-0.053200	4.815547
256.792518	8000.038405	12.604199	-0.053180	4.815557
256.838256	8000.031685	12.609203	-0.053189	4.815555
256.711405	8000.015736	12.614208	-0.053165	4.815551
257.016357	8000.044223	12.619213	-0.053222	4.815557
256.796088	8000.026748	12.624218	-0.053181	4.815553
256.745219	8000.061170	12.629223	-0.053172	4.815564
257.025224	8000.031576	12.634227	-0.053224	4.815554
257.081560	8000.028232	12.639232	-0.053234	4.815552
256.981535	8000.072531	12.644237	-0.053216	4.815566
256.857206	8000.047012	12.649242	-0.053193	4.815559
256.988174	8000.060908	12.654247	-0.053217	4.815562
256.911770	8000.047919	12.659251	-0.053203	4.815559
256.766559	8000.067984	12.664256	-0.053176	4.815566
256.886767	8000.049663	12.669261	-0.053199	4.815560
256.820034	8000.028289	12.674266	-0.053186	4.815554
256.794101	8000.049234	12.679271	-0.053182	4.815560
256.826901	8000.026281	12.684275	-0.053188	4.815553
256.967505	8000.056355	12.689280	-0.053214	4.815561
256.987982	8000.043881	12.694285	-0.053218	4.815557
256.833295	8000.031750	12.699290	-0.053189	4.815555
257.084543	8000.066836	12.704295	-0.053236	4.815564
257.047184	8000.013901	12.709299	-0.053229	4.815548
256.865971	8000.005608	12.714304	-0.053196	4.815547
256.939976	8000.051682	12.719309	-0.053210	4.815560
257.053911	7999.991607	12.724314	-0.053231	4.815542
256.913228	8000.020289	12.729319	-0.053205	4.815551
256.934891	8000.013175	12.734323	-0.053209	4.815549
256.955764	8000.029544	12.739328	-0.053213	4.815553
257.151449	8000.056246	12.744333	-0.053249	4.815560
256.743682	8000.030368	12.749338	-0.053174	4.815555
257.017575	8000.040191	12.754343	-0.053225	4.815556
256.881990	8000.042256	12.759347	-0.053199	4.815557
256.765382	8000.041427	12.764352	-0.053178	4.815558
256.944379	8000.052904	12.769357	-0.053211	4.815560
256.872807	8000.059219	12.774362	-0.053198	4.815562
256.907468	8000.051249	12.779367	-0.053205	4.815560
256.785673	8000.035383	12.784371	-0.053182	4.815556
257.036000	8000.049093	12.789376	-0.053229	4.815559
256.984851	8000.058946	12.794381	-0.053219	4.815562
256.822836	8000.007179	12.799386	-0.053189	4.815547
256.982066	8000.007652	12.804391	-0.053219	4.815547
257.172826	8000.011844	12.809395	-0.053255	4.815547
256.988727	7999.982145	12.814400	-0.053220	4.815539
257.175647	8000.065308	12.819405	-0.053255	4.815563
257.159755	8000.009519	12.824410	-0.053252	4.815547
257.003807	8000.073197	12.829415	-0.053223	4.815566
256.875912	8000.041211	12.834419	-0.053200	4.815557
257.064853	8000.048578	12.839424	-0.053235	4.815558
257.068182	8000.032620	12.844429	-0.053236	4.815554
256.891707	8000.040426	12.849434	-0.053203	4.815557
256.877255	8000.066898	12.854439	-0.053200	4.815565
257.038484	8000.057792	12.859443	-0.053230	4.815561
257.081841	8000.079869	12.864448	-0.053239	4.815567
257.054325	8000.059135	12.869453	-0.053234	4.815562
257.047152	8000.041938	12.874458	-0.053232	4.815557
257.096719	8000.056640	12.879463	-0.053242	4.815561
257.028736	8000.025633	12.884467	-0.053229	4.815552
257.121317	8000.055990	12.889472	-0.053246	4.815560
257.179480	8000.062289	12.894477	-0.053257	4.815562
256.891803	8000.022353	12.899482	-0.053204	4.815552
256.815067	8000.067032	12.904487	-0.053190	4.815565
256.966018	8000.052418	12.909491	-0.053218	4.815560
257.039573	8000.062172	12.914496	-0.053232	4.815562
257.167142	8000.058924	12.919501	-0.053256	4.815561
257.021718	8000.005292	12.924506	-0.053229	4.815546
257.091733	8000.053436	12.929511	-0.053242	4.815560
257.006078	8000.033889	12.934515	-0.053226	4.815554
256.905997	8000.064302	12.939520	-0.053207	4.815564
257.003395	8000.073378	12.944525	-0.053226	4.815566
256.913915	8000.023864	12.949530	-0.053209	4.815552
257.042207	8000.053736	12.954535	-0.053233	4.815560
257.078386	8000.053267	12.959539	-0.053240	4.815560
257.033928	8000.045073	12.964544	-0.053232	4.815557
257.054016	8000.061430	12.969549	-0.053235	4.815562
256.917483	8000.049595	12.974554	-0.053210	4.815559
257.002494	8000.079829	12.979559	-0.053226	4.815568
257.181173	8000.062464	12.984563	-0.053259	4.815562
257.055164	8000.037985	12.989568	-0.053236	4.815555
257.249756	8000.055056	12.994573	-0.053272	4.815559
257.063000	8000.035993	12.999578	-0.053238	4.815555
256.982672	8000.051777	13.004583	-0.053223	4.815560
256.982793	8000.046447	13.009587	-0.053223	4.815558
257.075232	8000.035149	13.014592	-0.053240	4.815554
256.994604	8000.069085	13.019597	-0.053225	4.815565
257.014205	8000.044849	13.024602	-0.053229	4.815557
257.089934	8000.039686	13.029607	-0.053243	4.815556
257.072563	8000.016982	13.034611	-0.053240	4.815549
256.930559	8000.011466	13.039616	-0.053214	4.815548
257.082933	8000.076977	13.044621	-0.053242	4.815567
257.093945	8000.059009	13.049626	-0.053244	4.815561
257.183132	8000.071154	13.054631	-0.053261	4.815564
257.246721	8000.039093	13.059635	-0.053273	4.815555
257.008695	8000.027736	13.064640	-0.053229	4.815552
256.943410	8000.064058	13.069645	-0.053217	4.815563
256.849070	8000.056117	13.074650	-0.053199	4.815562
256.985355	8000.070100	13.079655	-0.053225	4.815565
256.934722	8000.052192	13.084659	-0.053215	4.815560
256.798126	8000.065989	13.089664	-0.053190	4.815565
257.140150	8000.086538	13.094669	-0.053254	4.815569
256.861417	8000.058495	13.099674	-0.053202	4.815562
256.957520	8000.085706	13.104679	-0.053220	4.815570
256.985860	8000.057341	13.109683	-0.053225	4.815561
257.044123	8000.057233	13.114688	-0.053236	4.815561
257.150783	8000.069664	13.119693	-0.053256	4.815564
256.877949	8000.025698	13.124698	-0.053206	4.815552
257.184259	8000.062751	13.129703	-0.053263	4.815562
257.123937	8000.043617	13.134707	-0.053252	4.815557
256.929925	8000.046864	13.139712	-0.053215	4.815558
257.053261	8000.017914	13.144717	-0.053239	4.815549
257.030722	8000.019690	13.149722	-0.053234	4.815550
256.933684	8000.078990	13.154727	-0.053216	4.815568
256.979882	8000.038100	13.159731	-0.053225	4.815556
257.068137	8000.054503	13.164736	-0.053242	4.815560
257.175366	8000.076555	13.169741	-0.053262	4.815566
257.047722	8000.047777	13.174746	-0.053238	4.815558
257.170093	8000.055125	13.179751	-0.053261	4.815560
257.116455	8000.072413	13.184755	-0.053251	4.815565
257.001018	8000.058787	13.189760	-0.053230	4.815562
257.013763	8000.069684	13.194765	-0.053232	4.815565
257.023611	8000.039948	13.199770	-0.053234	4.815556
257.009275	8000.048266	13.204775	-0.053231	4.815558
257.013068	8000.019500	13.209779	-0.053232	4.815550
257.102910	8000.031656	13.214784	-0.053249	4.815553
257.006770	8000.058930	13.219789	-0.053231	4.815562
256.875836	8000.034371	13.224794	-0.053207	4.815555
256.928759	8000.070488	13.229799	-0.053217	4.815565
256.949467	8000.066562	13.234803	-0.053221	4.815564
256.748386	8000.031245	13.239808	-0.053184	4.815555
257.066309	8000.028971	13.244813	-0.053243	4.815552
257.015956	7999.998252	13.249818	-0.053234	4.815544
257.149925	8000.052782	13.254823	-0.053259	4.815559
257.121930	8000.041652	13.259827	-0.053253	4.815556
257.150172	8000.033578	13.264832	-0.053259	4.815553
257.232450	8000.058427	13.269837	-0.053274	4.815560
256.937618	8000.026917	13.274842	-0.053219	4.815552
256.970777	8000.043488	13.279847	-0.053226	4.815557
256.950675	8000.037827	13.284851	-0.053222	4.815556
256.742636	8000.021621	13.289856	-0.053183	4.815552
256.910897	8000.054282	13.294861	-0.053215	4.815561
257.036261	8000.014686	13.299866	-0.053238	4.815548
256.884643	8000.023965	13.304871	-0.053210	4.815552
257.091009	8000.008120	13.309875	-0.053249	4.815546
257.135201	8000.001374	13.314880	-0.053257	4.815544
257.197787	8000.038718	13.319885	-0.053269	4.815555
256.979442	8000.003118	13.324890	-0.053228	4.815545
257.099201	8000.038191	13.329895	-0.053251	4.815555
257.088151	8000.035883	13.334899	-0.053249	4.815554
256.879491	8000.047434	13.339904	-0.053210	4.815559
257.040656	8000.056484	13.344909	-0.053240	4.815561
257.090192	8000.012444	13.349914	-0.053249	4.815547
256.955086	8000.057238	13.354919	-0.053224	4.815561
256.899015	8000.013609	13.359923	-0.053214	4.815549
256.912684	8000.007433	13.364928	-0.053216	4.815547
256.944870	8000.025055	13.369933	-0.053223	4.815552
256.878725	8000.007962	13.374938	-0.053210	4.815547
257.039164	8000.082149	13.379943	-0.053240	4.815568
257.113662	8000.017157	13.384947	-0.053254	4.815549
256.840330	8000.040468	13.389952	-0.053203	4.815557
257.023934	8000.075516	13.394957	-0.053238	4.815566
256.938990	8000.032484	13.399962	-0.053222	4.815554
257.038615	8000.071500	13.404967	-0.053241	4.815565
256.941101	8000.019719	13.409971	-0.053223	4.815550
257.229466	8000.011622	13.414976	-0.053276	4.815547
257.174903	8000.023555	13.419981	-0.053266	4.815550
257.002608	7999.989775	13.424986	-0.053234	4.815541
256.843914	7999.992531	13.429991	-0.053205	4.815543
256.975341	8000.009639	13.434995	-0.053229	4.815547
257.124373	8000.012082	13.440000	-0.053257	4.815547
257.059264	8000.020638	13.445005	-0.053245	4.815550
256.958603	8000.022206	13.450010	-0.053227	4.815551
257.156058	8000.052141	13.455015	-0.053263	4.815559
257.059258	8000.005710	13.460019	-0.053245	4.815546
257.136702	8000.004848	13.465024	-0.053260	4.815545
257.058076	8000.028136	13.470029	-0.053245	4.815552
256.952871	8000.002929	13.475034	-0.053226	4.815545
256.965870	8000.045870	13.480039	-0.053229	4.815558
257.041629	8000.024687	13.485043	-0.053243	4.815551
257.091847	8000.018040	13.490048	-0.053252	4.815549
256.948443	8000.053086	13.495053	-0.053226	4.815560
257.013436	8000.031727	13.500058	-0.053238	4.815553
257.128913	8000.025078	13.505063	-0.053259	4.815551
257.205447	8000.014588	13.510067	-0.053274	4.815547
257.208371	8000.016780	13.515072	-0.053274	4.815548
257.197026	8000.046508	13.520077	-0.053272	4.815557
257.260821	8000.015518	13.525082	-0.053284	4.815547
257.275658	8000.057421	13.530087	-0.053287	4.815560
257.262112	8000.042256	13.535091	-0.053285	4.815555
257.090034	8000.013820	13.540096	-0.053253	4.815548
257.118325	8000.059147	13.545101	-0.053258	4.815561
257.281682	8000.032988	13.550106	-0.053289	4.815552
257.318019	8000.047474	13.555111	-0.053295	4.815557
257.013079	8000.037160	13.560115	-0.053239	4.815555
256.941754	7999.980466	13.565120	-0.053226	4.815539
257.279481	8000.030848	13.570125	-0.053289	4.815552
257.228897	7999.984105	13.575130	-0.053279	4.815538
257.204835	8000.031781	13.580135	-0.053275	4.815552
257.274861	8000.024389	13.585139	-0.053288	4.815550
257.280956	8000.034109	13.590144	-0.053289	4.815553
257.281343	8000.072573	13.595149	-0.053289	4.815564
257.126592	8000.041216	13.600154	-0.053261	4.815556
257.052113	8000.032531	13.605159	-0.053247	4.815553
257.070037	8000.045648	13.610163	-0.053250	4.815557
257.099383	8000.036524	13.615168	-0.053256	4.815554
257.215893	8000.071544	13.620173	-0.053278	4.815564
257.138599	8000.043589	13.625178	-0.053263	4.815556
257.176774	8000.057037	13.630183	-0.053271	4.815560
257.264561	8000.064888	13.635187	-0.053287	4.815562
257.201088	8000.040362	13.640192	-0.053275	4.815555
257.119352	8000.061463	13.645197	-0.053260	4.815562
256.970136	8000.013109	13.650202	-0.053232	4.815548
257.175053	8000.066662	13.655207	-0.053271	4.815563
257.161309	8000.063241	13.660211	-0.053268	4.815562
256.858625	8000.029468	13.665216	-0.053212	4.815553
257.189897	8000.067997	13.670221	-0.053274	4.815563
257.131053	8000.008302	13.675226	-0.053263	4.815546
257.115723	8000.046509	13.680231	-0.053260	4.815557
257.227787	8000.019511	13.685235	-0.053281	4.815549
257.266354	8000.025490	13.690240	-0.053288	4.815550
257.339127	8000.056592	13.695245	-0.053302	4.815559
257.286222	8000.043987	13.700250	-0.053292	4.815556
257.524316	8000.050022	13.705255	-0.053337	4.815556
257.197381	8000.013715	13.710259	-0.053276	4.815547
257.006670	8000.039444	13.715264	-0.053240	4.815556
257.207643	8000.044872	13.720269	-0.053278	4.815556
257.186241	8000.021034	13.725274	-0.053274	4.815549
257.230430	8000.022832	13.730279	-0.053282	4.815550
257.246793	8000.010291	13.735283	-0.053286	4.815546
257.076104	8000.034211	13.740288	-0.053254	4.815554
257.091495	8000.030199	13.745293	-0.053257	4.815552
257.103764	8000.004775	13.750298	-0.053259	4.815545
257.337928	8000.048126	13.755303	-0.053303	4.815557
257.266390	8000.014924	13.760307	-0.053290	4.815547
257.170956	8000.012305	13.765312	-0.053272	4.815547
257.230571	8000.015424	13.770317	-0.053283	4.815547
257.324930	8000.002021	13.775322	-0.053301	4.815543
257.116600	8000.054163	13.780327	-0.053262	4.815559
257.237361	8000.049736	13.785331	-0.053285	4.815557
257.152411	8000.038744	13.790336	-0.053269	4.815555
257.184702	8000.063844	13.795341	-0.053275	4.815562
257.048173	7999.998608	13.800346	-0.053250	4.815543
257.063856	8000.045866	13.805351	-0.053253	4.815557
257.114904	8000.033891	13.810355	-0.053262	4.815553
257.280069	8000.037666	13.815360	-0.053293	4.815554
257.384297	8000.041514	13.820365	-0.053313	4.815554
257.356077	8000.034653	13.825370	-0.053308	4.815552
257.239907	8000.058395	13.830375	-0.053286	4.815560
257.267318	8000.055647	13.835379	-0.053291	4.815559
257.294026	8000.044343	13.840384	-0.053296	4.815556
257.267951	8000.075966	13.845389	-0.053292	4.815565
257.264808	8000.037474	13.850394	-0.053291	4.815554
257.382337	8000.051151	13.855399	-0.053313	4.815557
257.268566	8000.040756	13.860403	-0.053292	4.815555
257.147063	8000.038779	13.865408	-0.053269	4.815555
257.253300	8000.074700	13.870413	-0.053289	4.815565
257.272081	8000.007729	13.875418	-0.053293	4.815545
257.242278	8000.018999	13.880423	-0.053287	4.815548
257.291283	8000.036896	13.885427	-0.053297	4.815553
257.138266	8000.019451	13.890432	-0.053268	4.815549
257.328397	8000.075968	13.895437	-0.053304	4.815565
257.129089	8000.050291	13.900442	-0.053267	4.815558
257.392665	8000.088783	13.905447	-0.053316	4.815568
257.537565	8000.051641	13.910451	-0.053343	4.815557
257.412462	8000.052809	13.915456	-0.053320	4.815557
257.503224	8000.063913	13.920461	-0.053337	4.815560
257.441248	8000.038344	13.925466	-0.053325	4.815553
257.438630	8000.089575	13.930471	-0.053325	4.815568
257.520269	8000.072760	13.935475	-0.053340	4.815563
257.530106	8000.053705	13.940480	-0.053342	4.815557
257.379659	8000.072615	13.945485	-0.053314	4.815563
257.232614	8000.055268	13.950490	-0.053287	4.815559
257.364000	8000.069171	13.955495	-0.053311	4.815562
257.580070	8000.057758	13.960499	-0.053352	4.815558
257.334409	8000.019575	13.965504	-0.053306	4.815548
257.432683	8000.047889	13.970509	-0.053325	4.815556
257.157064	8000.028442	13.975514	-0.053273	4.815552
257.258743	8000.026907	13.980519	-0.053292	4.815551
257.184761	8000.033183	13.985523	-0.053279	4.815553
257.260707	8000.063268	13.990528	-0.053293	4.815561
257.273276	8000.086979	13.995533	-0.053295	4.815568
257.150168	8000.042254	14.000538	-0.053272	4.815556
257.178840	8000.038459	14.005543	-0.053278	4.815554
257.466726	8000.025014	14.010547	-0.053332	4.815549
257.286007	8000.010321	14.015552	-0.053298	4.815546
257.420990	8000.052052	14.020557	-0.053323	4.815557
257.363740	8000.030832	14.025562	-0.053313	4.815551
257.339020	8000.042185	14.030567	-0.053308	4.815555
257.183764	8000.042860	14.035571	-0.053279	4.815556
257.377394	8000.050304	14.040576	-0.053316	4.815557
257.480413	8000.055200	14.045581	-0.053335	4.815558
257.383809	8000.042949	14.050586	-0.053317	4.815555
257.289348	8000.061707	14.055591	-0.053299	4.815561
257.309948	8000.066323	14.060595	-0.053303	4.815562
257.376572	8000.042856	14.065600	-0.053316	4.815555
257.377540	8000.080261	14.070605	-0.053316	4.815566
257.241931	8000.021447	14.075610	-0.053291	4.815549
257.145787	8000.057265	14.080615	-0.053273	4.815560
257.173090	8000.070536	14.085619	-0.053278	4.815564
257.144417	8000.020947	14.090624	-0.053273	4.815549
257.301020	8000.068371	14.095629	-0.053302	4.815562
257.120458	8000.008823	14.100634	-0.053269	4.815546
257.398161	8000.037934	14.105639	-0.053321	4.815553
257.497370	8000.045971	14.110643	-0.053339	4.815555
257.357934	8000.040497	14.115648	-0.053313	4.815554
257.293903	8000.040527	14.120653	-0.053301	4.815554
257.218727	8000.021150	14.125658	-0.053288	4.815549
257.351293	8000.042549	14.130663	-0.053312	4.815555
257.319664	8000.044176	14.135667	-0.053307	4.815555
257.154296	8000.029734	14.140672	-0.053276	4.815552
257.216830	8000.029696	14.145677	-0.053288	4.815552
257.096221	8000.019189	14.150682	-0.053265	4.815549
257.152857	8000.012646	14.155687	-0.053276	4.815547
257.410253	8000.020064	14.160691	-0.053324	4.815548
257.292470	7999.988243	14.165696	-0.053302	4.815539
257.412761	8000.028666	14.170701	-0.053325	4.815550
257.174921	8000.023720	14.175706	-0.053280	4.815550
257.358155	8000.022450	14.180711	-0.053315	4.815549
257.288739	8000.011712	14.185715	-0.053302	4.815546
257.369303	8000.009832	14.190720	-0.053317	4.815545
257.566010	8000.044027	14.195725	-0.053354	4.815554
257.392169	8000.017698	14.200730	-0.053321	4.815547
257.141273	8000.008267	14.205735	-0.053275	4.815546
257.288796	8000.052338	14.210739	-0.053302	4.815558
257.122224	8000.015448	14.215744	-0.053271	4.815548
257.131514	8000.077553	14.220749	-0.053273	4.815566
257.141474	8000.023255	14.225754	-0.053275	4.815550
257.287913	8000.018180	14.230759	-0.053302	4.815548
257.197460	8000.014574	14.235763	-0.053286	4.815547
257.171909	7999.963968	14.240768	-0.053281	4.815532
257.449399	8000.031523	14.245773	-0.053333	4.815551
257.451874	8000.034776	14.250778	-0.053333	4.815552
257.327864	8000.038098	14.255783	-0.053310	4.815553
257.328251	8000.031704	14.260787	-0.053310	4.815552
257.328979	7999.995411	14.265792	-0.053311	4.815541
257.453235	7999.673840	14.270797	-0.053334	4.815446

257.346427	7996.311434	14.275802	-0.053312	4.814464
257.474130	7990.745934	14.280807	-0.053332	4.812836
257.317589	7984.017890	14.285811	-0.053299	4.810868
257.161156	7976.652742	14.290816	-0.053265	4.808713
257.171874	7969.031323	14.295821	-0.053262	4.806482
257.141096	7961.184792	14.300826	-0.053251	4.804183
257.092207	7953.415243	14.305831	-0.053237	4.801907
257.174545	7945.421451	14.310835	-0.053247	4.799562
257.083206	7937.422583	14.315840	-0.053225	4.797216
257.059972	7929.419097	14.320845	-0.053216	4.794867
256.941532	7921.408609	14.325850	-0.053188	4.792515
256.956342	7913.404006	14.330855	-0.053186	4.790163
256.840432	7905.449283	14.335859	-0.053159	4.787826
256.748425	7897.341753	14.340864	-0.053137	4.785442
256.900592	7889.456984	14.345869	-0.053160	4.783121
256.964147	7881.417877	14.350874	-0.053167	4.780754
256.820209	7873.417072	14.355879	-0.053135	4.778398
256.819173	7865.441212	14.360883	-0.053130	4.776048
256.627248	7857.385306	14.365888	-0.053089	4.773674
256.657273	7849.397682	14.370893	-0.053089	4.771318
256.531637	7841.384555	14.375898	-0.053061	4.768953
256.420626	7833.414752	14.380903	-0.053035	4.766601
256.331635	7825.328750	14.385907	-0.053013	4.764212
256.374122	7817.425831	14.390912	-0.053016	4.761877
256.248431	7809.368589	14.395917	-0.052988	4.759494
256.228810	7801.388402	14.400922	-0.052979	4.757134
256.203574	7793.373112	14.405927	-0.052969	4.754761
256.134006	7785.291787	14.410931	-0.052951	4.752368
256.043364	7777.340746	14.415936	-0.052929	4.750013
256.030062	7769.343986	14.420941	-0.052921	4.747642
255.957509	7761.329559	14.425946	-0.052903	4.745265
255.864274	7753.355785	14.430951	-0.052880	4.742899
255.859394	7745.340674	14.435955	-0.052874	4.740520
255.720310	7737.359782	14.440960	-0.052843	4.738150
255.792584	7729.314647	14.445965	-0.052852	4.735758
255.751824	7721.318659	14.450970	-0.052839	4.733381
255.575617	7713.278227	14.455975	-0.052801	4.730990
255.495499	7705.306788	14.460979	-0.052781	4.728617
255.576910	7697.315689	14.465984	-0.052791	4.726237
255.443532	7689.306794	14.470989	-0.052761	4.723851
255.301251	7681.311353	14.475994	-0.052729	4.721468
255.403137	7673.293812	14.480999	-0.052743	4.719077
255.474011	7665.334441	14.486003	-0.052751	4.716702
255.207872	7657.284350	14.491008	-0.052697	4.714299
255.465167	7649.349163	14.496013	-0.052739	4.711928
255.354051	7641.259445	14.501018	-0.052714	4.709511
255.313847	7633.284066	14.506023	-0.052701	4.707126
255.385373	7625.310434	14.511027	-0.052709	4.704741
255.254902	7617.309158	14.516032	-0.052680	4.702346
255.200838	7609.304202	14.521037	-0.052665	4.699949
255.114079	7601.329185	14.526042	-0.052643	4.697560
254.938338	7593.290011	14.531047	-0.052605	4.695150
254.932059	7585.322710	14.536051	-0.052599	4.692761
254.764496	7577.207675	14.541056	-0.052563	4.690326
254.743880	7569.279722	14.546061	-0.052554	4.687946
254.505524	7561.248585	14.551066	-0.052504	4.685534
254.799538	7553.331589	14.556071	-0.052554	4.683154
254.676499	7545.317682	14.561075	-0.052526	4.680744
254.718505	7537.327478	14.566080	-0.052529	4.678340
254.555479	7529.308217	14.571085	-0.052493	4.675927
254.370778	7521.231919	14.576090	-0.052454	4.673494
254.265861	7513.130229	14.581095	-0.052429	4.671053
254.330723	7505.174362	14.586099	-0.052436	4.668655
254.215779	7497.228026	14.591104	-0.052409	4.666258
254.385433	7489.242484	14.596109	-0.052436	4.663848
254.392353	7481.261432	14.601114	-0.052432	4.661438
254.399226	7473.219425	14.606119	-0.052428	4.659008
254.200972	7465.280053	14.611123	-0.052386	4.656609
254.144809	7457.163668	14.616128	-0.052371	4.654154
254.185159	7449.220023	14.621133	-0.052373	4.651751
254.080400	7441.207900	14.626138	-0.052348	4.649325
253.958056	7433.234996	14.631143	-0.052320	4.646910
253.837695	7425.204502	14.636147	-0.052293	4.644477
253.835720	7417.265002	14.641152	-0.052287	4.642069
253.733895	7409.237861	14.646157	-0.052263	4.639634
253.592021	7401.238559	14.651162	-0.052232	4.637206
253.544438	7393.193305	14.656167	-0.052218	4.634763
253.486606	7385.194421	14.661171	-0.052202	4.632332
253.419615	7377.133022	14.666176	-0.052184	4.629882
253.553460	7369.191063	14.671181	-0.052204	4.627466
253.430475	7361.161709	14.676186	-0.052176	4.625022
253.426994	7353.203361	14.681191	-0.052170	4.622599
253.355785	7345.156960	14.686195	-0.052152	4.620148
253.248303	7337.196770	14.691200	-0.052127	4.617721
253.334787	7329.223435	14.696205	-0.052138	4.615289
253.283920	7321.180644	14.701210	-0.052123	4.612835
253.306840	7313.164631	14.706215	-0.052122	4.610388
253.186229	7305.197901	14.711219	-0.052095	4.607954
252.916930	7297.137500	14.716224	-0.052039	4.605491
253.136552	7289.209700	14.721229	-0.052075	4.603066
253.058288	7281.157782	14.726234	-0.052056	4.600603
252.926573	7273.205104	14.731239	-0.052026	4.598168
253.096327	7265.213459	14.736243	-0.052052	4.595721
252.824608	7257.103504	14.741248	-0.051997	4.593235
252.924262	7249.095090	14.746253	-0.052010	4.590780
252.784670	7241.087348	14.751258	-0.051979	4.588323
252.979062	7233.092364	14.756263	-0.052010	4.585869
252.728631	7225.150437	14.761267	-0.051958	4.583430
252.623334	7217.127139	14.766272	-0.051934	4.580965
252.509625	7209.172191	14.771277	-0.051907	4.578519
252.533714	7201.144018	14.776282	-0.051907	4.576049
252.297248	7193.118984	14.781287	-0.051858	4.573579
252.434678	7185.073804	14.786291	-0.051878	4.571102
252.302680	7177.111909	14.791296	-0.051848	4.568649
252.335962	7169.129425	14.796301	-0.051849	4.566188
252.437088	7161.104422	14.801306	-0.051863	4.563713
252.318661	7153.135225	14.806311	-0.051836	4.561253
252.228165	7145.134880	14.811315	-0.051814	4.558783
252.030880	7137.180823	14.816320	-0.051772	4.556325
251.987492	7129.134489	14.821325	-0.051759	4.553838
251.925890	7121.082574	14.826330	-0.051742	4.551347
252.121990	7113.101351	14.831335	-0.051774	4.548878
251.936413	7105.125421	14.836339	-0.051734	4.546408
251.767049	7097.046014	14.841344	-0.051697	4.543905
251.933227	7089.155499	14.846349	-0.051723	4.541459
251.734128	7081.128427	14.851354	-0.051681	4.538970
251.819164	7073.164462	14.856359	-0.051692	4.536498
251.894591	7065.109369	14.861363	-0.051701	4.533998
251.613637	7057.078093	14.866368	-0.051643	4.531502
251.733803	7049.069764	14.871373	-0.051660	4.529013
251.669835	7041.110222	14.876378	-0.051643	4.526538
251.516260	7033.115578	14.881383	-0.051610	4.524050
251.371298	7025.152405	14.886387	-0.051578	4.521571
251.199037	7017.099684	14.891392	-0.051540	4.519062
251.336243	7009.178323	14.896397	-0.051561	4.516593
251.506483	7001.077831	14.901402	-0.051587	4.514068
251.270433	6992.994084	14.906407	-0.051538	4.511545
251.161229	6985.046880	14.911411	-0.051513	4.509063
251.016017	6977.035462	14.916416	-0.051481	4.506560
251.256775	6969.057186	14.921421	-0.051520	4.504067
251.031097	6961.086356	14.926426	-0.051473	4.501574
250.977513	6953.056642	14.931431	-0.051458	4.499062
251.039561	6945.096176	14.936435	-0.051465	4.496570
251.041128	6937.028084	14.941440	-0.051460	4.494042
250.931762	6929.052239	14.946445	-0.051434	4.491542
250.919752	6921.023202	14.951450	-0.051427	4.489024
250.722077	6913.068177	14.956455	-0.051385	4.486528
250.713463	6905.071999	14.961459	-0.051378	4.484017
250.451493	6897.095854	14.966464	-0.051324	4.481511
250.537853	6889.038180	14.971469	-0.051335	4.478979
250.546090	6881.085126	14.976474	-0.051332	4.476478
250.255324	6873.012830	14.981479	-0.051272	4.473937
250.440257	6865.003387	14.986483	-0.051302	4.471416
250.574938	6856.995003	14.991488	-0.051322	4.468893
250.468018	6849.046364	14.996493	-0.051297	4.466388
250.221602	6841.027667	15.001498	-0.051246	4.463858
250.292285	6833.017753	15.006503	-0.051254	4.461331
250.285257	6825.039991	15.011507	-0.051247	4.458812
250.117141	6817.038102	15.016512	-0.051211	4.456283
250.403770	6809.030208	15.021517	-0.051259	4.453753
250.153837	6800.968437	15.026522	-0.051207	4.451203
249.969706	6793.021011	15.031527	-0.051168	4.448687
249.922413	6785.042856	15.036531	-0.051154	4.446161
249.651592	6776.990461	15.041536	-0.051099	4.443608
249.811428	6769.085681	15.046541	-0.051123	4.441103
249.689995	6761.016942	15.051546	-0.051095	4.438543
249.619597	6753.023016	15.056551	-0.051077	4.436006
249.647362	6744.962534	15.061555	-0.051077	4.433447
249.566850	6736.946557	15.066560	-0.051057	4.430900
249.720341	6728.968177	15.071565	-0.051081	4.428364
249.536557	6720.981586	15.076570	-0.051041	4.425823
249.533949	6712.945985	15.081575	-0.051036	4.423265
249.471752	6705.004141	15.086579	-0.051019	4.420736
249.486954	6696.955014	15.091584	-0.051017	4.418171
249.492668	6688.996855	15.096589	-0.051013	4.415634
249.287490	6680.984928	15.101594	-0.050969	4.413077
249.208693	6672.935649	15.106599	-0.050949	4.410507
249.378971	6664.951614	15.111603	-0.050976	4.407958
249.143986	6656.937677	15.116608	-0.050927	4.405396
249.082749	6648.991055	15.121613	-0.050911	4.402854
249.184058	6640.988805	15.126618	-0.050924	4.400295
248.867726	6633.012804	15.131623	-0.050860	4.397740
248.852432	6625.046211	15.136627	-0.050852	4.395188
248.667395	6616.953759	15.141632	-0.050813	4.392593
248.966174	6608.955101	15.146637	-0.050863	4.390029
248.758704	6600.954320	15.151642	-0.050820	4.387461
248.659017	6592.937935	15.156647	-0.050796	4.384887
248.868506	6584.985854	15.161651	-0.050830	4.382333
248.627410	6576.981442	15.166656	-0.050780	4.379759
248.687542	6569.029695	15.171661	-0.050786	4.377201
248.726372	6560.988903	15.176666	-0.050788	4.374614
248.691488	6552.975561	15.181671	-0.050776	4.372033
248.709116	6544.966950	15.186675	-0.050775	4.369453
248.698972	6536.951015	15.191680	-0.050768	4.366869
248.585277	6528.992143	15.196685	-0.050741	4.364300
248.268531	6521.059368	15.201690	-0.050677	4.361738
248.381588	6512.956724	15.206695	-0.050693	4.359122
248.323847	6505.051590	15.211699	-0.050677	4.356567
248.141104	6496.984720	15.216704	-0.050638	4.353957
248.075423	6488.855769	15.221709	-0.050621	4.351326
248.197612	6480.860963	15.226714	-0.050638	4.348739
248.023565	6472.906856	15.231719	-0.050601	4.346161
247.863237	6464.955333	15.236723	-0.050566	4.343582
247.721841	6456.946618	15.241728	-0.050534	4.340984
247.855146	6448.986943	15.246733	-0.050554	4.338402
247.825001	6440.959531	15.251738	-0.050543	4.335795
247.748491	6432.937967	15.256743	-0.050524	4.333188
248.029168	6424.924044	15.261747	-0.050571	4.330585
247.952905	6416.929401	15.266752	-0.050552	4.327983
247.632452	6408.947896	15.271757	-0.050487	4.325383
247.595200	6400.952532	15.276762	-0.050475	4.322779
247.522711	6392.927370	15.281767	-0.050456	4.320163
247.408476	6385.002809	15.286771	-0.050430	4.317578
247.193357	6376.904582	15.291776	-0.050385	4.314934
247.511971	6368.957739	15.296781	-0.050439	4.312341
247.575896	6360.887751	15.301786	-0.050446	4.309706
247.384894	6352.905065	15.306791	-0.050405	4.307095
247.405849	6344.933723	15.311795	-0.050404	4.304487
247.309351	6336.949041	15.316800	-0.050381	4.301873
247.269293	6328.902139	15.321805	-0.050368	4.299238
247.109935	6320.935482	15.326810	-0.050333	4.296626
247.079562	6312.898238	15.331815	-0.050323	4.293990
247.095343	6304.893346	15.336819	-0.050320	4.291364
246.954538	6296.843066	15.341824	-0.050289	4.288720
247.074275	6288.949944	15.346829	-0.050306	4.286128
246.858996	6280.897213	15.351834	-0.050261	4.283480
246.985366	6272.928155	15.356839	-0.050279	4.280860
247.004758	6264.946763	15.361843	-0.050278	4.278233
246.907762	6256.909783	15.366848	-0.050255	4.275586
246.854454	6248.898474	15.371853	-0.050240	4.272945
246.874899	6240.818270	15.376858	-0.050238	4.270281
246.626286	6232.880770	15.381863	-0.050187	4.267660
246.520086	6224.868827	15.386867	-0.050162	4.265014
246.510914	6216.904654	15.391872	-0.050155	4.262384
246.607109	6208.903848	15.396877	-0.050168	4.259740
246.340137	6200.912202	15.401882	-0.050113	4.257094
246.293441	6192.897910	15.406887	-0.050099	4.254441
246.316193	6184.899921	15.411891	-0.050099	4.251793
246.265732	6176.875983	15.416896	-0.050084	4.249134
246.170996	6168.919519	15.421901	-0.050061	4.246495
246.106790	6160.892872	15.426906	-0.050044	4.243831
246.029096	6152.887663	15.431911	-0.050025	4.241173
246.250036	6144.920316	15.436915	-0.050061	4.238528
245.965028	6136.909509	15.441920	-0.050002	4.235862
246.109069	6128.921467	15.446925	-0.050024	4.233207
246.165005	6120.873438	15.451930	-0.050029	4.230529
245.753032	6112.909824	15.456935	-0.049948	4.227873
245.802002	6104.935897	15.461939	-0.049952	4.225216
245.827849	6096.899337	15.466944	-0.049951	4.222536
245.649810	6088.925423	15.471949	-0.049913	4.219874
245.397458	6080.948577	15.476954	-0.049861	4.217208
245.505191	6072.929535	15.481959	-0.049876	4.214530
245.741991	6064.906948	15.486963	-0.049915	4.211850
245.505474	6056.874057	15.491968	-0.049866	4.209161
245.668729	6048.950598	15.496973	-0.049891	4.206510
245.518571	6040.907642	15.501978	-0.049858	4.203814
245.366202	6032.920266	15.506983	-0.049824	4.201136
245.486661	6024.940632	15.511987	-0.049842	4.198461
245.508595	6016.929174	15.516992	-0.049841	4.195772
245.461505	6008.855343	15.521997	-0.049827	4.193061
245.153865	6000.798832	15.527002	-0.049764	4.190350
245.101016	5992.850831	15.532007	-0.049749	4.187677
245.158386	5984.849628	15.537011	-0.049755	4.184986
244.981940	5976.929787	15.542016	-0.049717	4.182317
245.042414	5968.880384	15.547021	-0.049723	4.179606
244.919182	5960.951497	15.552026	-0.049695	4.176932
244.806676	5952.892311	15.557031	-0.049669	4.174212
244.812836	5944.874224	15.562035	-0.049665	4.171505
244.768317	5936.866744	15.567040	-0.049652	4.168800
244.842696	5928.886323	15.572045	-0.049660	4.166104
244.714573	5920.865331	15.577050	-0.049631	4.163389
244.733192	5912.902711	15.582055	-0.049630	4.160695
244.785581	5904.902616	15.587059	-0.049634	4.157986
244.565716	5896.872927	15.592064	-0.049588	4.155263
244.621860	5888.870295	15.597069	-0.049594	4.152550
244.475390	5880.836734	15.602074	-0.049561	4.149822
244.271620	5872.901533	15.607079	-0.049518	4.147125
244.361690	5864.869341	15.612083	-0.049530	4.144397
244.254477	5856.907252	15.617088	-0.049505	4.141689
244.346261	5848.871756	15.622093	-0.049517	4.138956
244.174420	5840.916098	15.627098	-0.049480	4.136246
244.025934	5832.852205	15.632103	-0.049447	4.133497
244.114384	5824.833662	15.637107	-0.049458	4.130764
244.017282	5816.827171	15.642112	-0.049435	4.128032
243.956014	5808.859456	15.647117	-0.049418	4.125311
244.081408	5800.891969	15.652122	-0.049437	4.122591
243.964295	5792.876600	15.657127	-0.049410	4.119850
243.829899	5784.933879	15.662131	-0.049380	4.117132
243.861203	5776.879916	15.667136	-0.049380	4.114376
243.744995	5768.867885	15.672141	-0.049353	4.111630
243.602230	5760.868642	15.677146	-0.049322	4.108887
243.631516	5752.860068	15.682151	-0.049322	4.106141
243.688064	5744.876720	15.687155	-0.049328	4.103402
243.621379	5736.869798	15.692160	-0.049310	4.100652
243.552317	5728.898346	15.697165	-0.049292	4.097911
243.472387	5720.918163	15.702170	-0.049272	4.095166
243.441724	5712.874330	15.707175	-0.049261	4.092398
243.372813	5704.874621	15.712179	-0.049243	4.089642
243.263595	5696.886457	15.717184	-0.049218	4.086889
243.448054	5688.900244	15.722189	-0.049247	4.084137
243.292306	5680.927457	15.727194	-0.049213	4.081384
243.214186	5672.954304	15.732199	-0.049193	4.078631
243.222357	5664.967751	15.737203	-0.049190	4.075871
243.021343	5656.903886	15.742208	-0.049147	4.073081
243.015828	5648.875592	15.747213	-0.049141	4.070303
242.943248	5640.898792	15.752218	-0.049122	4.067540
242.937112	5632.867974	15.757223	-0.049116	4.064758
243.046020	5624.925251	15.762227	-0.049131	4.062006
242.962450	5616.892377	15.767232	-0.049110	4.059218
243.019494	5608.976990	15.772237	-0.049116	4.056471
242.829895	5600.900261	15.777242	-0.049076	4.053662
242.835852	5592.880268	15.782247	-0.049072	4.050874
242.575139	5584.941628	15.787251	-0.049018	4.048109
242.544431	5576.880454	15.792256	-0.049007	4.045302
242.589645	5568.931862	15.797261	-0.049010	4.042534
242.432801	5560.920338	15.802266	-0.048976	4.039739
242.493628	5552.949826	15.807271	-0.048982	4.036959
242.338121	5544.908280	15.812275	-0.048948	4.034150
242.387699	5536.783124	15.817280	-0.048952	4.031312
242.547959	5528.839204	15.822285	-0.048977	4.028538
242.265719	5520.883445	15.827290	-0.048919	4.025750
242.306833	5512.886148	15.832295	-0.048922	4.022951
242.274969	5504.908312	15.837299	-0.048911	4.020156
242.193004	5496.910664	15.842304	-0.048890	4.017352
241.900978	5488.906627	15.847309	-0.048831	4.014539
241.930332	5480.885979	15.852314	-0.048831	4.011724
241.976363	5472.868431	15.857319	-0.048835	4.008908
241.947193	5464.906944	15.862323	-0.048824	4.006109
241.553431	5456.897443	15.867328	-0.048746	4.003285
241.729402	5448.918420	15.872333	-0.048773	4.000479
241.723671	5440.929297	15.877338	-0.048767	3.997665
241.558912	5432.881387	15.882343	-0.048731	3.994825
241.748762	5424.874273	15.887347	-0.048762	3.992003
241.467273	5416.838827	15.892352	-0.048704	3.989162
241.528885	5408.935543	15.897357	-0.048710	3.986371
241.451916	5400.887978	15.902362	-0.048691	3.983525
241.437766	5392.886491	15.907367	-0.048683	3.980694
241.479408	5384.948032	15.912371	-0.048686	3.977884
241.407333	5376.916589	15.917376	-0.048667	3.975037
241.351242	5368.906904	15.922381	-0.048652	3.972196
241.239423	5360.898593	15.927386	-0.048626	3.969353
241.057237	5352.934593	15.932391	-0.048587	3.966523
241.107750	5344.968720	15.937395	-0.048591	3.963693
240.952153	5336.960511	15.942400	-0.048557	3.960843
241.047327	5328.967070	15.947405	-0.048570	3.958000
240.894639	5320.965946	15.952410	-0.048536	3.955149
241.010716	5312.905899	15.957415	-0.048553	3.952279
241.190742	5304.921179	15.962419	-0.048581	3.949435
240.924877	5296.920304	15.967424	-0.048526	3.946575
240.832768	5288.969219	15.972429	-0.048504	3.943734
240.719892	5280.970792	15.977434	-0.048478	3.940873
240.681043	5272.967568	15.982439	-0.048466	3.938011
240.755986	5264.975849	15.987443	-0.048474	3.935152
240.704533	5256.950929	15.992448	-0.048460	3.932277
240.760936	5248.949125	15.997453	-0.048465	3.929410
240.511348	5240.983373	16.002458	-0.048413	3.926548
240.618714	5232.964598	16.007463	-0.048428	3.923672
240.573890	5224.999367	16.012467	-0.048415	3.920810
240.398224	5216.998904	16.017472	-0.048377	3.917931
240.340910	5209.001811	16.022477	-0.048361	3.915053
240.317781	5200.953389	16.027482	-0.048352	3.912155
240.261602	5192.923915	16.032487	-0.048336	3.909261
240.270720	5184.966284	16.037491	-0.048333	3.906392
239.845337	5176.956652	16.042496	-0.048248	3.903495
239.914160	5168.984407	16.047501	-0.048256	3.900617
239.892981	5160.992507	16.052506	-0.048247	3.897729
239.862547	5152.965607	16.057511	-0.048236	3.894826
239.798700	5144.963723	16.062515	-0.048219	3.891929
239.568121	5136.955980	16.067520	-0.048171	3.889025
239.801288	5128.990810	16.072525	-0.048210	3.886143
239.671779	5120.969061	16.077530	-0.048180	3.883231
239.686317	5112.944819	16.082535	-0.048178	3.880318
239.666747	5105.032394	16.087539	-0.048169	3.877444
239.491483	5096.969410	16.092544	-0.048131	3.874510
239.370096	5088.730405	16.097549	-0.048104	3.871510
239.322760	5080.839277	16.102554	-0.048090	3.868636
239.316879	5072.848134	16.107559	-0.048083	3.865725
239.255893	5064.934509	16.112563	-0.048067	3.862838
239.179936	5056.934427	16.117568	-0.048048	3.859917
239.258101	5048.995191	16.122573	-0.048057	3.857020
239.231475	5040.935319	16.127578	-0.048047	3.854074
238.968966	5032.956156	16.132583	-0.047993	3.851150
238.929454	5024.977576	16.137587	-0.047981	3.848230
239.004497	5016.942443	16.142592	-0.047990	3.845288
239.123548	5009.013131	16.147597	-0.048007	3.842384
238.777868	5001.016377	16.152602	-0.047937	3.839443
238.749936	4993.045372	16.157607	-0.047927	3.836516
238.846520	4985.060673	16.162611	-0.047940	3.833585
238.566618	4976.968490	16.167616	-0.047882	3.830604
238.582358	4969.004964	16.172621	-0.047880	3.827674
238.714896	4960.995088	16.177626	-0.047900	3.824727
238.634160	4953.028137	16.182631	-0.047880	3.821789
238.474513	4945.061747	16.187635	-0.047845	3.818847
238.607718	4937.055894	16.192640	-0.047865	3.815895
238.571390	4929.058415	16.197645	-0.047853	3.812940
238.370837	4921.020153	16.202650	-0.047810	3.809964
238.328170	4913.052434	16.207655	-0.047797	3.807016
238.354118	4905.061607	16.212659	-0.047797	3.804058
237.932482	4897.119298	16.217664	-0.047713	3.801105
238.136297	4889.096816	16.222669	-0.047746	3.798135
238.182912	4881.092351	16.227674	-0.047750	3.795165
238.105735	4873.014101	16.232679	-0.047730	3.792163
238.060350	4865.036945	16.237683	-0.047716	3.789197
238.130195	4857.019749	16.242688	-0.047724	3.786216
238.080597	4849.063781	16.247693	-0.047710	3.783253
237.885116	4841.058351	16.252698	-0.047669	3.780266
237.968316	4833.087724	16.257703	-0.047679	3.777295
238.041968	4825.052832	16.262707	-0.047687	3.774299
237.697635	4817.045493	16.267712	-0.047618	3.771300
237.765685	4809.069659	16.272717	-0.047626	3.768321
237.598753	4801.058570	16.277722	-0.047590	3.765320
237.417335	4793.114853	16.282727	-0.047551	3.762342
237.486162	4785.058842	16.287731	-0.047558	3.759325
237.565199	4777.080218	16.292736	-0.047568	3.756335
237.465248	4769.071591	16.297741	-0.047544	3.753328
237.389245	4761.069610	16.302746	-0.047525	3.750320
237.482548	4753.086793	16.307751	-0.047537	3.747322
237.283397	4745.059738	16.312755	-0.047495	3.744298
237.249845	4737.130016	16.317760	-0.047484	3.741312
237.206009	4729.114527	16.322765	-0.047470	3.738290
237.037730	4721.106766	16.327770	-0.047434	3.735267
237.086386	4713.087720	16.332775	-0.047438	3.732242
236.947734	4705.118436	16.337779	-0.047407	3.729228
236.866457	4697.118987	16.342784	-0.047387	3.726202
236.904302	4689.142400	16.347789	-0.047389	3.723186
236.700193	4681.177036	16.352794	-0.047346	3.720165
236.734540	4673.151871	16.357799	-0.047347	3.717124
236.827200	4665.165715	16.362803	-0.047359	3.714098
236.763662	4657.060459	16.367808	-0.047342	3.711020
236.578542	4649.096349	16.372813	-0.047302	3.707990
236.546704	4641.088656	16.377818	-0.047291	3.704945
236.293250	4633.156958	16.382823	-0.047239	3.701921
236.272572	4625.156825	16.387827	-0.047230	3.698874
236.371488	4617.149728	16.392832	-0.047243	3.695824
236.687583	4609.151289	16.397837	-0.047297	3.692781
236.345988	4601.155257	16.402842	-0.047228	3.689720
235.995649	4593.187016	16.407847	-0.047158	3.686667
236.263089	4585.190280	16.412851	-0.047203	3.683616
236.283349	4577.192850	16.417856	-0.047201	3.680556
236.029466	4569.234205	16.422861	-0.047149	3.677501
236.124279	4561.223961	16.427866	-0.047162	3.674432
235.883582	4553.210346	16.432871	-0.047112	3.671352
235.856277	4545.224970	16.437875	-0.047101	3.668284
235.824467	4537.149154	16.442880	-0.047090	3.665180
235.706738	4529.212580	16.447885	-0.047063	3.662124
235.830376	4521.200647	16.452890	-0.047081	3.659043
235.797892	4513.235196	16.457895	-0.047070	3.655973
235.826340	4505.218886	16.462899	-0.047070	3.652883
235.694502	4497.181512	16.467904	-0.047041	3.649777
235.536658	4489.253814	16.472909	-0.047006	3.646711
235.526990	4481.251627	16.477914	-0.046999	3.643617
235.631095	4473.229036	16.482919	-0.047013	3.640516
235.317994	4465.288052	16.487923	-0.046950	3.637432
235.381721	4457.252108	16.492928	-0.046957	3.634319
235.335393	4449.222642	16.497933	-0.046943	3.631203
235.005833	4441.238350	16.502938	-0.046876	3.628094
235.121463	4433.209015	16.507943	-0.046893	3.624977
235.373940	4425.257976	16.512947	-0.046935	3.621892
235.176613	4417.263489	16.517952	-0.046893	3.618774
235.245613	4409.278015	16.522957	-0.046901	3.615665
235.033718	4401.284049	16.527962	-0.046856	3.612542
234.987667	4393.250146	16.532967	-0.046842	3.609405
234.865769	4385.322122	16.537971	-0.046815	3.606305
234.783017	4377.302395	16.542976	-0.046794	3.603168
234.837913	4369.326903	16.547981	-0.046799	3.600048
234.769391	4361.373533	16.552986	-0.046781	3.596932
234.727963	4353.335975	16.557991	-0.046768	3.593780
234.694010	4345.348703	16.562995	-0.046757	3.590646
234.649975	4337.330213	16.568000	-0.046744	3.587496
234.672885	4329.324258	16.573005	-0.046743	3.584350
234.529346	4321.404069	16.578010	-0.046711	3.581231
234.511197	4313.354887	16.583015	-0.046703	3.578061
234.589730	4305.377852	16.588019	-0.046712	3.574920
234.369041	4297.366424	16.593024	-0.046666	3.571754
234.535154	4289.344854	16.598029	-0.046692	3.568592
234.434308	4281.367365	16.603034	-0.046668	3.565438
234.138502	4273.402706	16.608039	-0.046608	3.562279
234.177622	4265.421236	16.613043	-0.046610	3.559121
234.023428	4257.416290	16.618048	-0.046576	3.555946
234.144892	4249.351616	16.623053	-0.046593	3.552752
234.009638	4241.302296	16.628058	-0.046563	3.549553
233.970269	4233.327756	16.633063	-0.046551	3.546384
234.025444	4225.362692	16.638067	-0.046556	3.543219
233.863026	4217.379530	16.643072	-0.046520	3.540038
233.636801	4209.430372	16.648077	-0.046473	3.536865
233.893206	4201.390129	16.653082	-0.046516	3.533667
233.678642	4193.380235	16.658087	-0.046471	3.530465
233.655188	4185.417105	16.663091	-0.046461	3.527284
233.452054	4177.382745	16.668096	-0.046418	3.524066
233.532149	4169.468339	16.673101	-0.046428	3.520902
233.332721	4161.482676	16.678106	-0.046386	3.517697
233.409680	4153.438794	16.683111	-0.046395	3.514476
233.366390	4145.439513	16.688115	-0.046382	3.511265
233.078063	4137.433840	16.693120	-0.046323	3.508041
233.157854	4129.434366	16.698125	-0.046333	3.504828
233.214872	4121.488949	16.703130	-0.046338	3.501634
233.084511	4113.478533	16.708135	-0.046309	3.498404
233.157805	4105.538681	16.713139	-0.046318	3.495206
233.163948	4097.503020	16.718144	-0.046314	3.491964
233.194720	4089.503806	16.723149	-0.046314	3.488735
232.972567	4081.536476	16.728154	-0.046268	3.485508
232.833501	4073.543096	16.733159	-0.046237	3.482270
232.956339	4065.565073	16.738163	-0.046254	3.479043
232.658790	4057.626873	16.743168	-0.046194	3.475816
232.711021	4049.566925	16.748173	-0.046198	3.472548
232.821400	4041.540663	16.753178	-0.046214	3.469293
232.635948	4033.529332	16.758183	-0.046174	3.466031
232.675921	4025.543683	16.763187	-0.046177	3.462783
232.695431	4017.551058	16.768192	-0.046175	3.459529
232.653670	4009.601489	16.773197	-0.046162	3.456287
232.461105	4001.601163	16.778202	-0.046121	3.453017
232.492811	3993.552221	16.783207	-0.046122	3.449731
232.503703	3985.604230	16.788211	-0.046119	3.446483
232.371483	3977.593718	16.793216	-0.046089	3.443201
232.351832	3969.651868	16.798221	-0.046080	3.439948
232.238898	3961.655105	16.803226	-0.046054	3.436666
232.102922	3953.632173	16.808231	-0.046024	3.433369
232.029972	3945.641492	16.813235	-0.046005	3.430085
231.851298	3937.661856	16.818240	-0.045967	3.426798
231.890532	3929.647791	16.823245	-0.045969	3.423502
231.742026	3921.679622	16.828250	-0.045936	3.420215
231.625307	3913.671153	16.833255	-0.045909	3.416909
231.835854	3905.678948	16.838259	-0.045943	3.413618
231.759141	3897.663042	16.843264	-0.045924	3.410304
231.594323	3889.699271	16.848269	-0.045888	3.407005
231.708023	3881.689928	16.853274	-0.045904	3.403694
231.502236	3873.732338	16.858279	-0.045861	3.400390
231.515545	3865.804873	16.863283	-0.045858	3.397103
231.472724	3857.731179	16.868288	-0.045845	3.393750
231.369335	3849.672085	16.873293	-0.045821	3.390397
231.342656	3841.702324	16.878298	-0.045811	3.387081
231.224821	3833.698620	16.883303	-0.045784	3.383745
231.218997	3825.758525	16.888307	-0.045777	3.380436
231.195184	3817.770891	16.893312	-0.045768	3.377102
231.106354	3809.780997	16.898317	-0.045746	3.373763
231.077097	3801.754415	16.903322	-0.045736	3.370407
231.034112	3793.772817	16.908327	-0.045723	3.367066
231.027743	3785.808695	16.913331	-0.045716	3.363730
230.857340	3777.853909	16.918336	-0.045679	3.360388
230.989640	3769.859512	16.923341	-0.045699	3.357038
230.929037	3761.851789	16.928346	-0.045683	3.353672
230.784779	3753.814846	16.933351	-0.045651	3.350287
230.615544	3745.855719	16.938355	-0.045614	3.346931
230.451491	3737.845707	16.943360	-0.045578	3.343550
230.482865	3729.869045	16.948365	-0.045579	3.340186
230.431530	3721.885447	16.953370	-0.045564	3.336814
230.453410	3713.859253	16.958375	-0.045563	3.333422
230.415602	3705.858249	16.963379	-0.045551	3.330036
230.186684	3697.899864	16.968384	-0.045503	3.326657
230.403218	3689.903867	16.973389	-0.045539	3.323275
230.362492	3681.943003	16.978394	-0.045526	3.319895
230.159391	3673.973765	16.983399	-0.045483	3.316502
230.133044	3665.969248	16.988403	-0.045473	3.313097
230.099788	3657.909815	16.993408	-0.045462	3.309665
230.028453	3649.944163	16.998413	-0.045443	3.306268
230.078510	3641.951776	17.003418	-0.045447	3.302861
230.054202	3633.963297	17.008423	-0.045438	3.299449
229.785762	3626.046561	17.013427	-0.045383	3.296055
229.612143	3618.015115	17.018432	-0.045345	3.292611
229.911391	3609.987526	17.023437	-0.045396	3.289184
229.802843	3602.032558	17.028442	-0.045371	3.285769
229.496903	3594.051398	17.033447	-0.045308	3.282332
229.547548	3586.092961	17.038451	-0.045313	3.278914
229.482495	3578.098884	17.043456	-0.045296	3.275473
229.656230	3570.055312	17.048461	-0.045323	3.272016
229.425615	3562.072906	17.053466	-0.045275	3.268566
229.533135	3554.055170	17.058471	-0.045290	3.265111
229.517262	3546.096887	17.063475	-0.045282	3.261673
229.370422	3538.094064	17.068480	-0.045249	3.258206
229.386787	3530.131699	17.073485	-0.045247	3.254760
229.224851	3522.115684	17.078490	-0.045212	3.251280
229.051584	3514.125922	17.083495	-0.045174	3.247807
229.186520	3506.149364	17.088499	-0.045194	3.244349
229.049104	3498.193551	17.093504	-0.045164	3.240884
229.189656	3490.191840	17.098509	-0.045185	3.237408
228.975835	3482.179330	17.103514	-0.045140	3.233908
228.943963	3474.106420	17.108519	-0.045129	3.230386
228.716902	3466.179192	17.113523	-0.045081	3.226916
228.712035	3458.152721	17.118528	-0.045075	3.223407
228.789578	3450.211414	17.123533	-0.045085	3.219936
228.746296	3442.232290	17.128538	-0.045072	3.216439
228.490533	3434.234200	17.133543	-0.045019	3.212921
228.617960	3426.232301	17.138547	-0.045037	3.209413
228.568557	3418.243028	17.143552	-0.045023	3.205900
228.479835	3410.297470	17.148557	-0.045001	3.202400
228.483554	3402.302987	17.153562	-0.044997	3.198879
228.305233	3394.327546	17.158567	-0.044959	3.195355
228.380157	3386.318479	17.163571	-0.044968	3.191823
228.280161	3378.300352	17.168576	-0.044944	3.188276
228.174685	3370.313589	17.173581	-0.044919	3.184738
228.184369	3362.351485	17.178586	-0.044916	3.181212
228.248170	3354.354303	17.183591	-0.044923	3.177669
228.174413	3346.391907	17.188595	-0.044904	3.174131
228.191789	3338.372762	17.193600	-0.044902	3.170568
227.992372	3330.399011	17.198605	-0.044860	3.167012
227.839782	3322.437488	17.203610	-0.044826	3.163460
227.766459	3314.440905	17.208615	-0.044807	3.159891
227.835170	3306.478028	17.213619	-0.044815	3.156339
227.580951	3298.473160	17.218624	-0.044763	3.152751
227.712601	3290.409875	17.223629	-0.044782	3.149149
227.868473	3282.439761	17.228634	-0.044806	3.145586
227.685072	3274.456192	17.233639	-0.044767	3.141998
227.677800	3266.518056	17.238643	-0.044760	3.138434
227.546833	3258.508783	17.243648	-0.044731	3.134828
227.510633	3250.527187	17.248653	-0.044719	3.131235
227.225857	3242.547468	17.253658	-0.044661	3.127628
227.145709	3234.554772	17.258663	-0.044641	3.124019
227.260760	3226.593455	17.263667	-0.044657	3.120429
226.935274	3218.627731	17.268672	-0.044591	3.116814
227.201315	3210.581500	17.273677	-0.044636	3.113184
227.088863	3202.589164	17.278682	-0.044610	3.109558
227.055671	3194.601727	17.283687	-0.044598	3.105933
227.105484	3186.641429	17.288691	-0.044602	3.102320
226.915843	3178.673920	17.293696	-0.044562	3.098688
226.678135	3170.689839	17.298701	-0.044513	3.095043
226.622316	3162.699707	17.303706	-0.044497	3.091398
226.572885	3154.695817	17.308711	-0.044483	3.087744
226.831894	3146.682540	17.313715	-0.044526	3.084095
226.467248	3138.745203	17.318720	-0.044453	3.080447
226.586886	3130.760809	17.323725	-0.044470	3.076796
226.397962	3122.745754	17.328730	-0.044430	3.073113
226.292599	3114.666645	17.333735	-0.044405	3.069399
226.362166	3106.721397	17.338739	-0.044413	3.065751
226.289040	3098.750668	17.343744	-0.044394	3.062080
226.182293	3090.790273	17.348749	-0.044369	3.058407
226.114899	3082.828691	17.353754	-0.044352	3.054732
226.073223	3074.809900	17.358759	-0.044339	3.051026
226.387587	3066.812098	17.363763	-0.044392	3.047343
225.867983	3058.873501	17.368768	-0.044290	3.043644
225.801922	3050.912728	17.373773	-0.044273	3.039950
225.896816	3042.954399	17.378778	-0.044285	3.036262
225.804713	3034.911621	17.383783	-0.044263	3.032520
225.615138	3026.940598	17.388787	-0.044223	3.028803
225.639791	3018.915607	17.393792	-0.044222	3.025066
225.895448	3010.931936	17.398797	-0.044265	3.021356
225.754749	3002.978680	17.403802	-0.044233	3.017635
225.570275	2994.987171	17.408807	-0.044194	3.013890
225.620800	2986.995689	17.413811	-0.044198	3.010152
225.657339	2979.002931	17.418816	-0.044200	3.006407
225.468675	2971.055807	17.423821	-0.044160	3.002669
225.449038	2963.080254	17.428826	-0.044151	2.998921
225.201374	2955.103644	17.433831	-0.044100	2.995156
225.107782	2947.089741	17.438835	-0.044077	2.991376
225.287898	2939.064246	17.443840	-0.044106	2.987600
225.203794	2931.101342	17.448845	-0.044085	2.983836
225.244798	2923.127948	17.453850	-0.044087	2.980068
225.148200	2915.172052	17.458855	-0.044064	2.976296
225.295976	2907.157386	17.463859	-0.044087	2.972505
224.922826	2899.186964	17.468864	-0.044012	2.968703
224.865363	2891.195050	17.473869	-0.043996	2.964902
224.789797	2883.248144	17.478874	-0.043977	2.961116
224.735953	2875.262610	17.483879	-0.043962	2.957309
224.698919	2867.294732	17.488883	-0.043950	2.953505
224.582336	2859.262787	17.493888	-0.043923	2.949662
224.672609	2851.269856	17.498893	-0.043935	2.945844
224.532612	2843.325242	17.503898	-0.043904	2.942032
224.480547	2835.325497	17.508903	-0.043889	2.938193
224.526633	2827.359991	17.513907	-0.043892	2.934370
224.279289	2819.351827	17.518912	-0.043841	2.930506
224.153972	2811.397406	17.523917	-0.043813	2.926670
224.216249	2803.409013	17.528922	-0.043819	2.922822
224.204949	2795.416550	17.533927	-0.043812	2.918964
224.327894	2787.467688	17.538931	-0.043830	2.915128
224.229935	2779.369164	17.543936	-0.043806	2.911203
224.149771	2771.396167	17.548941	-0.043786	2.907334
224.195410	2763.445656	17.553946	-0.043790	2.903478
223.850842	2755.498105	17.558951	-0.043720	2.899598
223.974740	2747.531292	17.563955	-0.043738	2.895728
223.722563	2739.541875	17.568960	-0.043686	2.891821
223.750667	2731.548862	17.573965	-0.043686	2.887923
223.764297	2723.596975	17.578970	-0.043684	2.884038
223.648412	2715.605193	17.583975	-0.043657	2.880122
223.525600	2707.668421	17.588979	-0.043629	2.876227
223.308512	2699.653808	17.593984	-0.043584	2.872283
223.538627	2691.639559	17.598989	-0.043621	2.868359
223.400048	2683.671851	17.603994	-0.043591	2.864432
223.322658	2675.706994	17.608999	-0.043571	2.860504
223.534444	2667.735079	17.614003	-0.043605	2.856583
223.255993	2659.744698	17.619008	-0.043548	2.852621
223.167634	2651.777503	17.624013	-0.043527	2.848675
223.303465	2643.792223	17.629018	-0.043547	2.844727
223.219577	2635.827788	17.634023	-0.043526	2.840772
223.057091	2627.886562	17.639027	-0.043491	2.836818
222.808419	2619.891043	17.644032	-0.043440	2.832827
222.794933	2611.871965	17.649037	-0.043432	2.828832
222.838444	2603.885857	17.654042	-0.043435	2.824851
222.611856	2595.935642	17.659047	-0.043388	2.820866
222.746796	2587.957841	17.664051	-0.043408	2.816883
222.632171	2579.957624	17.669056	-0.043381	2.812869
222.609864	2571.958895	17.674061	-0.043372	2.808855
222.661988	2563.982287	17.679066	-0.043377	2.804851
222.542073	2556.018909	17.684071	-0.043349	2.800838
222.477068	2548.086051	17.689075	-0.043332	2.796837
222.472233	2540.072902	17.694080	-0.043326	2.792794
222.545954	2532.070893	17.699085	-0.043334	2.788755
222.328560	2524.121031	17.704090	-0.043289	2.784719
222.166103	2516.171495	17.709095	-0.043254	2.780681
222.177425	2508.197974	17.714099	-0.043251	2.776635
222.139347	2500.198866	17.719104	-0.043238	2.772568
222.199535	2492.201252	17.724109	-0.043244	2.768501
222.000555	2484.259785	17.729114	-0.043202	2.764441
222.018863	2476.281381	17.734119	-0.043201	2.760369
221.978248	2468.341188	17.739123	-0.043188	2.756307
221.826168	2460.271072	17.744128	-0.043155	2.752166
221.852585	2452.251158	17.749133	-0.043154	2.748056
221.809689	2444.289076	17.754138	-0.043141	2.743964
221.647507	2436.343295	17.759143	-0.043106	2.739868
221.681660	2428.411059	17.764147	-0.043107	2.735784
221.496490	2420.416280	17.769152	-0.043068	2.731649
221.353837	2412.444961	17.774157	-0.043036	2.727522
221.453097	2404.466633	17.779162	-0.043049	2.723400
221.369483	2396.483602	17.784167	-0.043029	2.719258
221.429774	2388.553899	17.789171	-0.043035	2.715146
221.159916	2380.563433	17.794176	-0.042979	2.710976
221.119357	2372.577114	17.799181	-0.042967	2.706816
221.230442	2364.596262	17.804186	-0.042982	2.702662
221.006597	2356.648160	17.809191	-0.042936	2.698498
220.984100	2348.681054	17.814195	-0.042926	2.694329
220.894353	2340.668886	17.819200	-0.042904	2.690127
220.856070	2332.698747	17.824205	-0.042892	2.685943
220.776485	2324.747230	17.829210	-0.042872	2.681760
220.710314	2316.773343	17.834215	-0.042855	2.677559
220.611719	2308.796409	17.839219	-0.042831	2.673348
220.512366	2300.796736	17.844224	-0.042808	2.669119
220.475570	2292.805722	17.849229	-0.042796	2.664891
220.557507	2284.874186	17.854234	-0.042806	2.660696
220.329185	2276.895380	17.859239	-0.042758	2.656448
220.308615	2268.939279	17.864243	-0.042749	2.652220
220.225204	2260.935575	17.869248	-0.042729	2.647955
220.311777	2252.966967	17.874253	-0.042740	2.643714
220.126891	2245.033063	17.879258	-0.042700	2.639466
220.053606	2237.055711	17.884263	-0.042682	2.635195
220.161077	2229.059436	17.889267	-0.042696	2.630919
220.047582	2221.088260	17.894272	-0.042670	2.626636
219.841302	2213.129145	17.899277	-0.042627	2.622345
219.853718	2205.172311	17.904282	-0.042624	2.618063
219.790970	2197.208299	17.909287	-0.042607	2.613765
219.801994	2189.207528	17.914291	-0.042604	2.609446
219.492744	2181.259274	17.919296	-0.042541	2.605126
219.693080	2173.280156	17.924301	-0.042574	2.600816
219.660368	2165.334899	17.929306	-0.042562	2.596502
219.502400	2157.233178	17.934311	-0.042528	2.592087
219.440683	2149.221514	17.939315	-0.042511	2.587720
219.345723	2141.276471	17.944320	-0.042488	2.583380
219.363094	2133.348705	17.949325	-0.042487	2.579049
219.455013	2125.394370	17.954330	-0.042499	2.574702
219.379637	2117.415596	17.959335	-0.042480	2.570323
219.299496	2109.480882	17.964339	-0.042460	2.565960
219.239245	2101.529408	17.969344	-0.042443	2.561582
219.253006	2093.570021	17.974349	-0.042441	2.557197
218.911458	2085.635123	17.979354	-0.042372	2.552793
218.976798	2077.610002	17.984359	-0.042379	2.548360
219.120504	2069.642896	17.989363	-0.042401	2.543957
218.910207	2061.708990	17.994368	-0.042356	2.539540
218.677412	2053.765503	17.999373	-0.042308	2.535108
218.873540	2045.761094	18.004378	-0.042339	2.530665
218.584743	2037.815030	18.009383	-0.042281	2.526212
218.452133	2029.870953	18.014387	-0.042251	2.521763
218.437293	2021.916944	18.019392	-0.042243	2.517310
218.555584	2013.920415	18.024397	-0.042260	2.512834
218.322266	2005.939436	18.029402	-0.042211	2.508334
218.055916	1997.972187	18.034407	-0.042157	2.503830
218.116182	1990.023192	18.039411	-0.042163	2.499353
218.004286	1982.066747	18.044416	-0.042137	2.494851
217.912099	1974.081659	18.049421	-0.042115	2.490326
217.989649	1966.116090	18.054426	-0.042124	2.485816
217.952359	1958.168848	18.059431	-0.042112	2.481300
217.961719	1950.209465	18.064435	-0.042108	2.476773
217.810707	1942.253494	18.069440	-0.042075	2.472227
217.869470	1934.251020	18.074445	-0.042081	2.467661
217.701058	1926.318880	18.079450	-0.042045	2.463111
217.565556	1918.362635	18.084455	-0.042014	2.458541
217.677024	1910.407107	18.089459	-0.042030	2.453981
217.562585	1902.421104	18.094464	-0.042004	2.449378
217.360891	1894.461641	18.099469	-0.041961	2.444775
217.405391	1886.518653	18.104474	-0.041964	2.440192
217.388973	1878.562729	18.109479	-0.041956	2.435587
217.238515	1870.560709	18.114483	-0.041923	2.430937
217.017504	1862.581263	18.119488	-0.041877	2.426286
217.181421	1854.607046	18.124493	-0.041902	2.421659
217.121230	1846.679531	18.129498	-0.041886	2.417033
217.062977	1838.703960	18.134503	-0.041870	2.412369
217.068897	1830.746766	18.139507	-0.041866	2.407713
216.982591	1822.795688	18.144512	-0.041845	2.403044
216.958289	1814.853967	18.149517	-0.041835	2.398376
216.928957	1806.908783	18.154522	-0.041824	2.393697
216.872014	1798.918059	18.159527	-0.041809	2.388979
216.748674	1790.978950	18.164531	-0.041781	2.384277
216.557140	1783.035747	18.169536	-0.041740	2.379558
216.631773	1775.069000	18.174541	-0.041749	2.374837
216.584226	1767.095906	18.179546	-0.041735	2.370093
216.356560	1759.154149	18.184551	-0.041687	2.365344
216.373544	1751.209600	18.189555	-0.041685	2.360603
216.467213	1743.256817	18.194560	-0.041698	2.355854
216.416301	1735.264615	18.199565	-0.041683	2.351059
216.234310	1727.312201	18.204570	-0.041644	2.346269
216.068152	1719.360775	18.209575	-0.041608	2.341470
216.121760	1711.424092	18.214579	-0.041613	2.336688
215.848633	1703.476816	18.219584	-0.041557	2.331864
216.009268	1695.482194	18.224589	-0.041582	2.327036
215.987185	1687.546695	18.229594	-0.041573	2.322219
215.715763	1679.621196	18.234599	-0.041517	2.317377
215.893729	1671.656346	18.239603	-0.041545	2.312539
215.888614	1663.682031	18.244608	-0.041539	2.307670
215.756349	1655.744016	18.249613	-0.041509	2.302801
215.613442	1647.818986	18.254618	-0.041478	2.297930
215.471617	1639.857915	18.259623	-0.041446	2.293026
215.551678	1631.893528	18.264627	-0.041456	2.288128
215.356689	1623.957025	18.269632	-0.041415	2.283213
215.356862	1616.002709	18.274637	-0.041410	2.278294
215.271273	1608.056288	18.279642	-0.041389	2.273361
215.227149	1600.022010	18.284647	-0.041375	2.268367
215.202881	1592.089603	18.289651	-0.041366	2.263427
215.086346	1584.155841	18.294656	-0.041339	2.258467
215.068014	1576.207962	18.299661	-0.041330	2.253495
214.942462	1568.249505	18.304666	-0.041302	2.248497
214.928959	1560.298901	18.309671	-0.041294	2.243503
214.859150	1552.391200	18.314675	-0.041276	2.238519
214.779215	1544.446206	18.319680	-0.041256	2.233500
214.796497	1536.469002	18.324685	-0.041254	2.228457
214.879802	1528.531816	18.329690	-0.041265	2.223435
214.706052	1520.594087	18.334695	-0.041227	2.218378
214.658255	1512.665917	18.339699	-0.041213	2.213326
214.606834	1504.699439	18.344704	-0.041199	2.208239
214.549136	1496.763441	18.349709	-0.041183	2.203158
214.447242	1488.853472	18.354714	-0.041159	2.198078
214.383515	1480.884618	18.359719	-0.041142	2.192953
214.021632	1472.958960	18.364723	-0.041069	2.187815
213.947150	1465.009004	18.369728	-0.041050	2.182676
213.835059	1457.063387	18.374733	-0.041024	2.177525
214.113314	1449.082595	18.379738	-0.041071	2.172374
213.942990	1441.142872	18.384743	-0.041034	2.167196
213.899547	1433.224720	18.389747	-0.041021	2.162032
213.779060	1425.297354	18.394752	-0.040994	2.156842
213.763796	1417.352197	18.399757	-0.040986	2.151638
213.813308	1409.395609	18.404762	-0.040990	2.146420
213.666368	1401.458981	18.409767	-0.040957	2.141183
213.549624	1393.540361	18.414771	-0.040931	2.135949
213.501164	1385.584726	18.419776	-0.040917	2.130684
213.458522	1377.643467	18.424781	-0.040904	2.125415
213.426665	1369.723406	18.429786	-0.040893	2.120149
213.301920	1361.811387	18.434791	-0.040864	2.114866
213.223217	1353.791412	18.439795	-0.040844	2.109502
213.023408	1345.869693	18.444800	-0.040802	2.104178
213.076269	1337.940616	18.449805	-0.040807	2.098861
213.097089	1330.011663	18.454810	-0.040806	2.093526
212.983623	1322.062075	18.459815	-0.040780	2.088152
213.030252	1314.136013	18.464819	-0.040783	2.082795
212.897649	1306.242129	18.469824	-0.040753	2.077428
212.653170	1298.317396	18.474829	-0.040703	2.072015
212.814195	1290.349540	18.479834	-0.040728	2.066599
212.541767	1282.453466	18.484839	-0.040672	2.061174
212.335525	1274.558442	18.489843	-0.040628	2.055743
212.210717	1266.608509	18.494848	-0.040600	2.050267
212.267761	1258.644377	18.499853	-0.040606	2.044786
212.194116	1250.750972	18.504858	-0.040587	2.039325
212.038531	1242.829136	18.509863	-0.040553	2.033822
212.161933	1234.843303	18.514867	-0.040571	2.028287
211.861445	1226.947492	18.519872	-0.040510	2.022757
211.814484	1219.023985	18.524877	-0.040496	2.017218
211.850521	1211.081264	18.529882	-0.040498	2.011659
211.809701	1203.136087	18.534887	-0.040485	2.006075
211.654861	1195.248317	18.539891	-0.040451	2.000504
211.740262	1187.314941	18.544896	-0.040462	1.994911
211.671035	1179.375644	18.549901	-0.040444	1.989281
211.665894	1171.461382	18.554906	-0.040438	1.983659
211.650343	1163.538253	18.559911	-0.040430	1.978015
211.726953	1155.601712	18.564915	-0.040439	1.972354
211.510717	1147.695283	18.569920	-0.040394	1.966667
211.535911	1139.785294	18.574925	-0.040393	1.960987
211.477567	1131.891649	18.579930	-0.040377	1.955294
211.368028	1123.912858	18.584935	-0.040352	1.949516
211.387931	1115.998986	18.589939	-0.040351	1.943783
211.166606	1108.098162	18.594944	-0.040304	1.938016
211.178030	1100.177624	18.599949	-0.040301	1.932242
211.066974	1092.265506	18.604954	-0.040276	1.926444
210.934545	1084.370719	18.609959	-0.040246	1.920639
210.862504	1076.475922	18.614963	-0.040227	1.914823
210.637711	1068.562781	18.619968	-0.040181	1.908958
210.471576	1060.664803	18.624973	-0.040145	1.903094
210.719318	1052.715682	18.629978	-0.040186	1.897219
210.629170	1044.795599	18.634983	-0.040164	1.891310
210.615188	1036.884553	18.639987	-0.040156	1.885398
210.532644	1029.000214	18.644992	-0.040136	1.879479
210.418882	1021.112547	18.649997	-0.040109	1.873536
210.324929	1013.187026	18.655002	-0.040087	1.867547
210.262728	1005.268731	18.660007	-0.040070	1.861548
210.334630	997.367357	18.665011	-0.040079	1.855558
210.455332	989.426826	18.670016	-0.040096	1.849525
210.149572	981.570357	18.675021	-0.040034	1.843486
210.158671	973.678073	18.680026	-0.040031	1.837436
209.907336	965.788372	18.685031	-0.039979	1.831338
209.894473	957.868414	18.690035	-0.039971	1.825225
209.843457	949.987889	18.695040	-0.039957	1.819117
209.722495	942.091681	18.700045	-0.039929	1.812968
209.526019	934.217212	18.705050	-0.039888	1.806805
209.384592	926.321977	18.710055	-0.039856	1.800612
209.596087	918.403469	18.715059	-0.039890	1.794422
209.536286	910.446912	18.720064	-0.039874	1.788148
209.277733	902.587213	18.725069	-0.039821	1.781904
209.359033	894.691789	18.730074	-0.039831	1.775651
209.266309	886.800259	18.735079	-0.039809	1.769357
209.085532	878.950184	18.740083	-0.039770	1.763064
208.950884	871.083160	18.745088	-0.039740	1.756740
208.840862	863.186278	18.750093	-0.039715	1.750372
208.845072	855.305907	18.755098	-0.039710	1.744008
208.606686	847.436697	18.760103	-0.039661	1.737600
208.724383	839.527812	18.765107	-0.039678	1.731181
208.609109	831.653012	18.770112	-0.039651	1.724736
208.464789	823.809991	18.775117	-0.039619	1.718289
208.533882	815.898882	18.780122	-0.039627	1.711789
208.296043	808.019482	18.785127	-0.039578	1.705251
208.162175	800.180193	18.790131	-0.039548	1.698734
208.113248	792.286874	18.795136	-0.039534	1.692159
208.167044	784.382617	18.800141	-0.039539	1.685562
208.100806	776.540090	18.805146	-0.039521	1.678975
207.923395	768.682518	18.810151	-0.039483	1.672335
208.077375	760.781545	18.815155	-0.039507	1.665676
208.027418	752.920509	18.820160	-0.039493	1.658996
207.850704	745.080950	18.825165	-0.039455	1.652291
207.801304	737.217911	18.830170	-0.039440	1.645556
207.656610	729.380679	18.835175	-0.039408	1.638802
207.679611	721.487129	18.840179	-0.039408	1.631994
207.538496	713.592799	18.845184	-0.039376	1.625134
207.588977	705.737366	18.850189	-0.039381	1.618307
207.660773	697.873754	18.855194	-0.039389	1.611445
207.379909	690.052510	18.860199	-0.039332	1.604543
207.263072	682.238974	18.865203	-0.039305	1.597640
207.164942	674.379878	18.870208	-0.039282	1.590669
207.010816	666.546412	18.875213	-0.039248	1.583683
206.858865	658.731556	18.880218	-0.039215	1.576682
206.894081	650.847312	18.885223	-0.039216	1.569615
206.778196	643.027545	18.890227	-0.039190	1.562553
206.693177	635.202741	18.895232	-0.039169	1.555458
206.620610	627.342096	18.900237	-0.039150	1.548300
206.684871	619.494074	18.905242	-0.039157	1.541140
206.529808	611.674029	18.910247	-0.039123	1.533940
206.352126	603.856467	18.915251	-0.039085	1.526704
206.359890	596.027409	18.920256	-0.039082	1.519452
206.239477	588.217540	18.925261	-0.039054	1.512163
206.122943	580.399797	18.930266	-0.039028	1.504832
206.026026	572.587336	18.935271	-0.039004	1.497473
205.761683	564.795180	18.940275	-0.038950	1.490072
205.818747	556.963924	18.945280	-0.038956	1.482645
205.856855	549.144163	18.950285	-0.038958	1.475190
205.892736	541.272261	18.955290	-0.038960	1.467646
205.668933	533.484311	18.960295	-0.038913	1.460103
205.578272	525.707164	18.965299	-0.038891	1.452553
205.731450	517.859185	18.970304	-0.038915	1.444933
205.437470	510.125215	18.975309	-0.038855	1.437312
205.373135	502.330257	18.980314	-0.038838	1.429628
205.113745	494.556237	18.985319	-0.038785	1.421891
205.248816	486.750741	18.990323	-0.038805	1.414145
205.223984	478.949480	18.995328	-0.038795	1.406335
204.975004	471.214239	19.000333	-0.038744	1.398510
205.106916	463.397902	19.005338	-0.038763	1.390622
204.892370	455.637441	19.010343	-0.038719	1.382688
204.734819	447.895470	19.015347	-0.038684	1.374737
204.758767	440.098300	19.020352	-0.038684	1.366713
204.585880	432.363029	19.025357	-0.038647	1.358673
204.636812	424.591919	19.030362	-0.038651	1.350586
204.463250	416.843769	19.035367	-0.038614	1.342435
204.575203	409.075014	19.040371	-0.038630	1.334263
204.291387	401.356314	19.045376	-0.038572	1.326023
204.221855	393.631401	19.050381	-0.038554	1.317764
204.278518	385.772410	19.055386	-0.038560	1.309330
204.198765	378.011186	19.060391	-0.038540	1.300924
203.997302	370.329989	19.065395	-0.038497	1.292527
203.698586	362.642844	19.070400	-0.038437	1.284051
203.841152	354.900377	19.075405	-0.038458	1.275540
203.705219	347.205819	19.080410	-0.038428	1.266972
203.591274	339.505543	19.085415	-0.038402	1.258344
203.436889	331.824616	19.090419	-0.038368	1.249671
203.579099	324.093997	19.095424	-0.038390	1.240937
203.253573	316.450535	19.100429	-0.038324	1.232150
203.115866	308.765088	19.105434	-0.038294	1.223289
202.967719	301.090977	19.110439	-0.038261	1.214374
202.773762	293.432173	19.115443	-0.038220	1.205401
202.774869	285.761088	19.120448	-0.038216	1.196386
202.691070	278.092926	19.125453	-0.038195	1.187289
202.757021	270.424662	19.130458	-0.038202	1.178152
202.557095	262.791198	19.135463	-0.038160	1.168931
202.662799	255.138676	19.140467	-0.038175	1.159677
202.501448	247.498239	19.145472	-0.038140	1.150307
202.093815	239.907516	19.150477	-0.038059	1.140869
202.011581	232.297398	19.155482	-0.038039	1.131398
201.847577	224.688981	19.160487	-0.038004	1.121831
201.907094	217.073654	19.165491	-0.038010	1.112222
201.619754	209.508312	19.170496	-0.037952	1.102517
201.240938	201.974275	19.175501	-0.037876	1.092746
201.323744	194.370573	19.180506	-0.037887	1.082899
200.923186	186.854442	19.185511	-0.037808	1.072967
200.784962	179.290713	19.190515	-0.037777	1.062939
200.365287	171.790857	19.195520	-0.037694	1.052836
199.982444	164.288373	19.200525	-0.037618	1.042640
199.751209	156.786308	19.205530	-0.037570	1.032379
199.517970	149.273082	19.210535	-0.037522	1.022000
199.242199	141.796736	19.215539	-0.037466	1.011555
198.524327	134.400287	19.220544	-0.037327	1.001005
198.365360	126.894414	19.225549	-0.037293	0.990325
198.011136	119.441478	19.230554	-0.037222	0.979556
197.583638	112.017313	19.235559	-0.037138	0.968690
197.421224	104.579445	19.240563	-0.037103	0.957749
196.996664	97.195487	19.245568	-0.037019	0.946693
196.460755	89.843484	19.250573	-0.036915	0.935525
196.062194	82.482791	19.255578	-0.036836	0.924246
195.495833	75.163015	19.260583	-0.036726	0.912844
194.990198	67.840403	19.265587	-0.036627	0.901310
194.536842	60.760721	19.270592	-0.036538	0.890027