Thu Mar 11 20:58:38 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.900704	-0.184069	0.000000	-0.000061	0.722123

0.588268	-0.154543	0.005005	-0.000003	0.722072
0.927442	-0.209534	0.010010	-0.000066	0.722083
0.964713	-0.220662	0.015014	-0.000073	0.722074
0.862633	-0.199665	0.020019	-0.000054	0.722080
0.836976	-0.195733	0.025024	-0.000050	0.722079
0.886502	-0.207254	0.030029	-0.000059	0.722074
1.127731	-0.245719	0.035034	-0.000104	0.722083
0.731882	-0.176625	0.040038	-0.000030	0.722080
0.630884	-0.158483	0.045043	-0.000012	0.722081
0.661841	-0.162963	0.050048	-0.000017	0.722083
0.606292	-0.157563	0.055053	-0.000007	0.722074
0.683922	-0.166141	0.060058	-0.000022	0.722085
0.958345	-0.218702	0.065062	-0.000073	0.722078
0.895332	-0.372938	0.070067	-0.000061	0.721753
0.803305	-0.355361	0.075072	-0.000044	0.721755
1.153247	-0.421885	0.080077	-0.000109	0.721747
1.144144	-0.416333	0.085082	-0.000108	0.721755
0.771806	-0.354084	0.090086	-0.000038	0.721747
0.786302	-0.354402	0.095091	-0.000041	0.721752
0.876044	-0.496143	0.100096	-0.000058	0.721505
0.774099	-0.511498	0.105101	-0.000039	0.721439
0.709557	-0.495838	0.110106	-0.000027	0.721447
0.848705	-0.523078	0.115110	-0.000053	0.721443
0.771298	-0.510566	0.120115	-0.000039	0.721440
0.683062	-0.617107	0.125120	-0.000022	0.721200
0.797238	-0.678750	0.130125	-0.000044	0.721119
0.812054	-0.675715	0.135130	-0.000046	0.721130
0.579988	-0.636971	0.140134	-0.000003	0.721125
0.556132	-0.689305	0.145139	0.000001	0.721014
0.579573	-0.759336	0.150144	-0.000003	0.720885
0.705051	-0.782594	0.155149	-0.000027	0.720883
0.812542	-0.798999	0.160154	-0.000047	0.720889
0.795693	-0.907373	0.165158	-0.000044	0.720670
0.628654	-0.942024	0.170163	-0.000013	0.720543
0.613827	-0.936609	0.175168	-0.000010	0.720549
0.768094	-1.005078	0.180173	-0.000039	0.720468
0.647432	-1.102548	0.185178	-0.000016	0.720234
0.458068	-1.071521	0.190182	0.000019	0.720229
0.703086	-1.126848	0.195187	-0.000027	0.720206
0.848324	-1.303757	0.200192	-0.000054	0.719909
0.505502	-1.246389	0.205197	0.000010	0.719902
0.369385	-1.234667	0.210202	0.000035	0.719877
0.448846	-1.387319	0.215206	0.000020	0.719604
0.525332	-1.399239	0.220211	0.000006	0.719608
0.148723	-1.374338	0.225216	0.000076	0.719525
-0.069697	-1.465440	0.230221	0.000117	0.719269
0.287229	-1.523151	0.235226	0.000050	0.719280
0.217522	-1.580906	0.240230	0.000063	0.719142
-0.027573	-1.626677	0.245235	0.000109	0.718966
0.169601	-1.658907	0.250240	0.000072	0.718972
0.382522	-1.826257	0.255245	0.000032	0.718717
0.391675	-1.859842	0.260250	0.000030	0.718654
0.331457	-1.903924	0.265254	0.000042	0.718546
0.283439	-1.989069	0.270259	0.000051	0.718361
0.069808	-1.950547	0.275264	0.000090	0.718362
0.211558	-2.149603	0.280269	0.000064	0.718019
0.235382	-2.150252	0.285274	0.000059	0.718026
-0.703542	-2.100780	0.290278	0.000234	0.717794
-1.464481	-2.007387	0.295283	0.000376	0.717710
-1.308840	-2.039020	0.300288	0.000347	0.717703
-1.805114	-2.114044	0.305293	0.000439	0.717380
-3.153461	-1.870996	0.310298	0.000690	0.717386
-3.686072	-1.779524	0.315302	0.000789	0.717379
-2.810675	-2.012926	0.320307	0.000626	0.717226
-3.097137	-2.030721	0.325312	0.000679	0.717090
-3.000839	-2.051702	0.330317	0.000661	0.717083
-4.036721	-1.887665	0.335322	0.000854	0.717043
-3.997941	-2.040085	0.340326	0.000847	0.716755
-3.988257	-2.041694	0.345331	0.000845	0.716755
-3.870153	-2.060879	0.350336	0.000823	0.716759
-4.421403	-2.034968	0.355341	0.000925	0.716616
-5.201717	-1.976712	0.360346	0.001070	0.716456
-4.983867	-2.017057	0.365350	0.001030	0.716453
-5.046201	-2.008044	0.370355	0.001041	0.716449
-4.585963	-2.133702	0.375360	0.000956	0.716363
-5.806672	-2.032980	0.380365	0.001183	0.716132
-6.125563	-1.972314	0.385370	0.001242	0.716140
-5.769958	-2.039247	0.390374	0.001176	0.716133
-5.703508	-2.050534	0.395379	0.001163	0.716134
-5.908502	-2.116998	0.400384	0.001201	0.715930
-6.999859	-1.948386	0.405389	0.001404	0.715879
-6.400310	-2.049400	0.410394	0.001293	0.715891
-6.769887	-1.986166	0.415398	0.001361	0.715886
-6.877817	-1.966586	0.420403	0.001381	0.715887
-7.063537	-2.096407	0.425408	0.001416	0.715564
-7.036680	-2.110090	0.430413	0.001411	0.715547
-7.123232	-2.092508	0.435418	0.001427	0.715551
-7.706091	-1.990646	0.440422	0.001535	0.715547
-7.363258	-2.063767	0.445427	0.001471	0.715524
-7.977606	-2.099910	0.450432	0.001586	0.715235
-8.293442	-2.046676	0.455437	0.001645	0.715229
-8.358225	-2.030218	0.460442	0.001656	0.715239
-8.184286	-2.064197	0.465446	0.001624	0.715233
-8.422689	-2.021452	0.470451	0.001668	0.715234
-8.373471	-2.117802	0.475456	0.001659	0.715061
-9.277023	-2.033067	0.480461	0.001827	0.714909
-8.910606	-2.095829	0.485466	0.001759	0.714915
-9.079574	-2.065965	0.490470	0.001790	0.714914
-8.989714	-2.082565	0.495475	0.001774	0.714913
-8.805393	-2.123191	0.500480	0.001739	0.714898
-10.245323	-2.012312	0.505485	0.002007	0.714609
-10.210295	-2.016156	0.510490	0.002000	0.714614
-9.785287	-2.094076	0.515494	0.001921	0.714610
-10.072185	-2.043320	0.520499	0.001975	0.714609
-10.376275	-1.985372	0.525504	0.002031	0.714617
-10.048671	-2.047945	0.530509	0.001970	0.714609
-9.800008	-2.193896	0.535514	0.001924	0.714407
-11.298660	-1.989110	0.540518	0.002203	0.714284
-11.192537	-2.010298	0.545523	0.002183	0.714279
-10.549617	-2.122209	0.550528	0.002063	0.714285
-11.090080	-2.031070	0.555533	0.002164	0.714274
-11.104878	-2.024309	0.560538	0.002166	0.714283
-10.796448	-2.102836	0.565542	0.002109	0.714236
-11.954060	-2.027884	0.570547	0.002324	0.713975
-11.580293	-2.092671	0.575552	0.002255	0.713979
-11.831542	-2.051130	0.580557	0.002301	0.713973
-11.954924	-2.027304	0.585562	0.002324	0.713977
-12.044977	-2.011261	0.590566	0.002341	0.713977
-12.121181	-1.998943	0.595571	0.002355	0.713975
-11.613093	-2.149752	0.600576	0.002260	0.713855
-13.098623	-1.985913	0.605581	0.002537	0.713655
-12.705167	-2.052718	0.610586	0.002463	0.713661
-12.568298	-2.078637	0.615590	0.002438	0.713658
-12.763328	-2.045736	0.620595	0.002474	0.713655
-12.827995	-2.029662	0.625600	0.002486	0.713664
-13.107636	-1.985298	0.630605	0.002538	0.713654
-12.741996	-2.113056	0.635610	0.002470	0.713529
-13.781543	-2.008807	0.640614	0.002663	0.713368
-13.802992	-2.008009	0.645619	0.002667	0.713362
-13.430849	-2.071098	0.650624	0.002598	0.713369
-13.642839	-2.036273	0.655629	0.002637	0.713363
-13.604657	-2.038211	0.660634	0.002630	0.713373
-13.609508	-2.040645	0.665638	0.002631	0.713367
-13.893815	-2.091965	0.670643	0.002684	0.713164
-14.752979	-2.004904	0.675648	0.002844	0.713033
-14.571365	-2.043187	0.680653	0.002810	0.713021
-14.395589	-2.068703	0.685658	0.002777	0.713033
-14.770586	-2.003734	0.690662	0.002847	0.713029
-14.598432	-2.035703	0.695667	0.002814	0.713027
-14.270817	-2.091842	0.700672	0.002753	0.713032
-14.852217	-2.077628	0.705677	0.002862	0.712854
-15.907555	-1.957501	0.710682	0.003058	0.712719
-15.234246	-2.078609	0.715686	0.002933	0.712717
-15.303565	-2.066808	0.720691	0.002945	0.712716
-15.736973	-1.988018	0.725696	0.003026	0.712719
-16.006424	-1.943420	0.730701	0.003076	0.712712
-15.263636	-2.072400	0.735706	0.002938	0.712719
-15.231759	-2.120890	0.740710	0.002932	0.712634
-16.392521	-2.034818	0.745715	0.003148	0.712394
-15.894871	-2.119417	0.750720	0.003055	0.712402
-16.504067	-2.017532	0.755725	0.003168	0.712389
-16.438742	-2.025334	0.760730	0.003156	0.712397
-16.082908	-2.092070	0.765734	0.003090	0.712390
-16.408021	-2.036102	0.770739	0.003150	0.712387
-16.277418	-2.120498	0.775744	0.003126	0.712265
-17.333324	-2.020414	0.780749	0.003322	0.712090
-16.761452	-2.117929	0.785754	0.003216	0.712099
-17.063509	-2.065440	0.790758	0.003272	0.712096
-17.605112	-1.972030	0.795763	0.003373	0.712090
-17.074818	-2.061863	0.800768	0.003274	0.712100
-17.091546	-2.063271	0.805773	0.003277	0.712091
-17.575528	-2.070514	0.810778	0.003367	0.711905
-18.237095	-2.022285	0.815782	0.003490	0.711766
-17.981455	-2.068858	0.820787	0.003442	0.711764
-17.960356	-2.068665	0.825792	0.003438	0.711772
-18.499905	-1.977184	0.830797	0.003539	0.711763
-18.059464	-2.051401	0.835802	0.003457	0.711772
-17.735094	-2.111473	0.840806	0.003396	0.711768
-18.385313	-2.063725	0.845811	0.003517	0.711632
-19.014714	-2.035598	0.850816	0.003634	0.711464
-18.666300	-2.101638	0.855821	0.003569	0.711457
-19.174697	-2.007094	0.860826	0.003664	0.711465
-19.184477	-2.006449	0.865830	0.003666	0.711463
-19.081772	-2.026983	0.870835	0.003646	0.711458
-18.833931	-2.068410	0.875840	0.003600	0.711464
-19.172684	-2.045065	0.880845	0.003663	0.711390
-19.858551	-2.044512	0.885850	0.003791	0.711148
-19.697378	-2.073548	0.890854	0.003761	0.711147
-20.365311	-1.956286	0.895859	0.003885	0.711144
-19.697171	-2.070499	0.900864	0.003760	0.711154
-19.628055	-2.088567	0.905869	0.003747	0.711142
-20.042676	-2.011517	0.910874	0.003825	0.711149
-19.899498	-2.058271	0.915878	0.003798	0.711107
-20.570468	-2.054025	0.920883	0.003923	0.710877
-20.272598	-2.103941	0.925888	0.003867	0.710883
-21.104246	-1.961842	0.930893	0.004022	0.710871
-20.548786	-2.056136	0.935898	0.003918	0.710881
-20.244977	-2.111920	0.940902	0.003862	0.710878
-20.856605	-2.006291	0.945907	0.003976	0.710871
-20.809273	-2.090803	0.950912	0.003967	0.710719
-21.691962	-2.025548	0.955917	0.004131	0.710536
-21.342087	-2.084031	0.960922	0.004066	0.710544
-21.556025	-2.048448	0.965926	0.004105	0.710539
-21.882163	-1.993418	0.970931	0.004166	0.710533
-21.344725	-2.083841	0.975936	0.004066	0.710543
-21.760054	-2.016043	0.980941	0.004143	0.710531
-21.816182	-2.065123	0.985946	0.004154	0.710413
-22.498727	-2.037794	0.990950	0.004281	0.710225
-22.490974	-2.041561	0.995955	0.004279	0.710220
-22.341334	-2.065379	1.000960	0.004251	0.710226
-22.609200	-2.021590	1.005965	0.004301	0.710219
-22.627645	-2.015337	1.010970	0.004304	0.710225
-22.414891	-2.051926	1.015974	0.004265	0.710227
-22.443796	-2.096966	1.020979	0.004270	0.710127
-23.102566	-2.090192	1.025984	0.004392	0.709906
-23.365798	-2.048358	1.030989	0.004441	0.709896
-23.706883	-1.984958	1.035994	0.004505	0.709902
-23.100751	-2.095207	1.040998	0.004392	0.709897
-23.515079	-2.023400	1.046003	0.004469	0.709894
-23.693750	-1.988126	1.051008	0.004502	0.709901
-23.427315	-2.059347	1.056013	0.004452	0.709853
-23.839955	-2.113561	1.061018	0.004529	0.709598
-24.139188	-2.060312	1.066022	0.004585	0.709598
-24.583002	-1.983015	1.071027	0.004667	0.709595
-24.026640	-2.076590	1.076032	0.004564	0.709606
-24.337467	-2.025685	1.081037	0.004621	0.709597
-24.239469	-2.041318	1.086042	0.004603	0.709601
-24.156547	-2.100271	1.091046	0.004588	0.709513
-25.482493	-1.989855	1.096051	0.004834	0.709261
-24.932330	-2.082682	1.101056	0.004732	0.709272
-25.344938	-2.014804	1.106061	0.004809	0.709260
-25.542893	-1.974378	1.111066	0.004845	0.709271
-25.352140	-2.010483	1.116070	0.004810	0.709267
-25.215309	-2.037329	1.121075	0.004784	0.709262
-24.903146	-2.088675	1.126080	0.004726	0.709271
-25.734412	-2.080215	1.131085	0.004881	0.708991
-26.473643	-1.964960	1.136090	0.005018	0.708959
-26.048020	-2.041014	1.141094	0.004939	0.708958
-25.876489	-2.073771	1.146099	0.004907	0.708954
-26.267261	-1.998396	1.151104	0.004980	0.708966
-26.071885	-2.037080	1.156109	0.004943	0.708958
-25.853133	-2.074120	1.161114	0.004902	0.708962
-26.284574	-2.105440	1.166118	0.004983	0.708746
-27.334978	-1.972051	1.171123	0.005178	0.708638
-26.848960	-2.051038	1.176128	0.005087	0.708654
-27.080520	-2.014641	1.181133	0.005130	0.708644
-27.220049	-1.987982	1.186138	0.005156	0.708648
-26.705197	-2.080292	1.191142	0.005060	0.708647
-27.051086	-2.020518	1.196147	0.005125	0.708643
-27.056786	-2.093498	1.201152	0.005126	0.708495
-27.773416	-2.036870	1.206157	0.005259	0.708353
-27.769218	-2.034777	1.211162	0.005258	0.708359
-27.854343	-2.019530	1.216166	0.005274	0.708359
-27.733903	-2.043608	1.221171	0.005251	0.708354
-27.163275	-2.141965	1.226176	0.005145	0.708361
-27.969897	-2.003733	1.231181	0.005295	0.708350
-28.648223	-2.030235	1.236186	0.005421	0.708055
-28.502484	-2.075213	1.241190	0.005394	0.708017
-28.558451	-2.068083	1.246195	0.005405	0.708011
-28.540771	-2.067771	1.251200	0.005401	0.708018
-28.766533	-2.031545	1.256205	0.005443	0.708010
-28.731598	-2.033998	1.261210	0.005437	0.708018
-28.436995	-2.084134	1.266214	0.005382	0.708023
-29.366639	-2.070906	1.271219	0.005555	0.707717
-29.637887	-2.027503	1.276224	0.005605	0.707708
-29.867167	-1.992126	1.281229	0.005648	0.707697
-29.931886	-1.977052	1.286234	0.005660	0.707704
-29.567410	-2.041746	1.291238	0.005592	0.707705
-29.739020	-2.015091	1.296243	0.005624	0.707697
-29.769586	-2.004781	1.301248	0.005629	0.707707
-29.680351	-2.077695	1.306253	0.005612	0.707593
-30.540997	-2.029369	1.311258	0.005773	0.707382
-30.218799	-2.087346	1.316262	0.005713	0.707381
-30.833681	-1.980277	1.321267	0.005827	0.707376
-30.280850	-2.076446	1.326272	0.005724	0.707381
-30.373573	-2.063111	1.331277	0.005741	0.707375
-31.141425	-1.925626	1.336282	0.005884	0.707376
-30.538988	-2.054557	1.341286	0.005772	0.707333
-31.040374	-2.091842	1.346291	0.005865	0.707079
-31.205316	-2.058751	1.351296	0.005896	0.707087
-31.602776	-1.990550	1.356301	0.005970	0.707082
-31.139428	-2.071939	1.361306	0.005883	0.707084
-31.064147	-2.086721	1.366310	0.005869	0.707082
-31.529822	-2.005390	1.371315	0.005956	0.707078
-31.356757	-2.122580	1.376320	0.005923	0.706905
-32.307239	-2.030731	1.381325	0.006100	0.706750
-32.291434	-2.032541	1.386330	0.006097	0.706752
-31.985256	-2.087043	1.391334	0.006040	0.706752
-32.534097	-1.991545	1.396339	0.006142	0.706748
-32.356769	-2.016978	1.401344	0.006109	0.706760
-32.293123	-2.031823	1.406349	0.006097	0.706753
-32.224606	-2.105122	1.411354	0.006084	0.706631
-33.468548	-1.973901	1.416358	0.006316	0.706449
-33.606080	-1.953893	1.421363	0.006341	0.706440
-33.350125	-1.992258	1.426368	0.006294	0.706455
-33.157971	-2.030942	1.431373	0.006258	0.706446
-33.550246	-1.960397	1.436378	0.006331	0.706448
-33.478875	-1.972346	1.441382	0.006317	0.706449
-33.101861	-2.044215	1.446387	0.006247	0.706440
-33.391788	-2.101897	1.451392	0.006301	0.706220
-34.485549	-1.952975	1.456397	0.006505	0.706128
-34.119890	-2.016025	1.461402	0.006436	0.706132
-33.579663	-2.111552	1.466406	0.006336	0.706134
-34.121563	-2.018450	1.471411	0.006437	0.706127
-34.021941	-2.032950	1.476416	0.006418	0.706134
-33.937585	-2.050902	1.481421	0.006402	0.706128
-34.729937	-2.021453	1.486426	0.006550	0.705904
-34.713682	-2.042517	1.491430	0.006547	0.705867
-34.664451	-2.054711	1.496435	0.006537	0.705861
-34.837095	-2.018854	1.501440	0.006569	0.705871
-35.142811	-1.967929	1.506445	0.006626	0.705864
-34.810905	-2.027331	1.511450	0.006564	0.705864
-34.742148	-2.052087	1.516454	0.006551	0.705839
-35.764641	-2.025241	1.521459	0.006742	0.705526
-35.817248	-2.011560	1.526464	0.006751	0.705535
-36.070786	-1.971058	1.531469	0.006799	0.705526
-36.133540	-1.958051	1.536474	0.006810	0.705530
-35.973715	-1.985537	1.541478	0.006780	0.705532
-35.822825	-2.017288	1.546483	0.006752	0.705522
-35.690266	-2.037081	1.551488	0.006727	0.705530
-36.313876	-2.030901	1.556493	0.006843	0.705319
-36.935977	-1.972269	1.561498	0.006959	0.705214
-36.286950	-2.085028	1.566502	0.006838	0.705220
-36.455794	-2.059583	1.571507	0.006870	0.705211
-36.622681	-2.024640	1.576512	0.006901	0.705221
-36.460313	-2.057504	1.581517	0.006870	0.705214
-36.722944	-2.010687	1.586522	0.006919	0.705214
-37.119787	-2.099954	1.591526	0.006993	0.704892
-37.291844	-2.072732	1.596531	0.007025	0.704885
-37.492958	-2.031689	1.601536	0.007062	0.704896
-37.387152	-2.053964	1.606541	0.007042	0.704889
-37.306302	-2.068420	1.611546	0.007027	0.704889
-37.441399	-2.041276	1.616550	0.007052	0.704895
-37.919665	-2.011544	1.621555	0.007141	0.704784
-38.475598	-2.005299	1.626560	0.007245	0.704597
-37.995641	-2.095788	1.631565	0.007155	0.704587
-38.268502	-2.045518	1.636570	0.007206	0.704590
-38.452848	-2.010100	1.641574	0.007240	0.704596
-38.436207	-2.014193	1.646579	0.007237	0.704593
-38.026329	-2.087462	1.651584	0.007161	0.704593
-38.524332	-2.085709	1.656589	0.007253	0.704418
-39.391861	-2.009457	1.661594	0.007415	0.704260
-38.790063	-2.113808	1.666598	0.007303	0.704266
-39.124685	-2.057290	1.671603	0.007365	0.704260
-39.350963	-2.013002	1.676608	0.007407	0.704268
-39.102144	-2.060695	1.681613	0.007361	0.704262
-39.110462	-2.059486	1.686618	0.007362	0.704261
-39.424356	-2.116793	1.691622	0.007420	0.704033
-40.491236	-1.969040	1.696627	0.007619	0.703948
-40.157964	-2.022811	1.701632	0.007557	0.703959
-40.097576	-2.036948	1.706637	0.007545	0.703952
-40.284316	-2.003580	1.711642	0.007580	0.703953
-39.710967	-2.104681	1.716646	0.007473	0.703955
-39.949839	-2.063799	1.721651	0.007518	0.703952
-40.416436	-2.097812	1.726656	0.007605	0.703716
-40.917752	-2.047428	1.731661	0.007698	0.703637
-40.872341	-2.055682	1.736666	0.007689	0.703637
-40.879103	-2.051810	1.741670	0.007690	0.703642
-41.155502	-2.009419	1.746675	0.007742	0.703629
-40.614323	-2.099063	1.751680	0.007641	0.703643
-40.942157	-2.044175	1.756685	0.007702	0.703636
-42.002480	-1.998681	1.761690	0.007899	0.703346
-41.727209	-2.047415	1.766694	0.007848	0.703347
-41.852573	-2.028121	1.771699	0.007871	0.703341
-41.858929	-2.023279	1.776704	0.007872	0.703349
-41.792488	-2.037642	1.781709	0.007860	0.703344
-41.579141	-2.077075	1.786714	0.007820	0.703341
-41.513084	-2.089127	1.791718	0.007808	0.703341
-42.584556	-2.063877	1.796723	0.008007	0.703006
-42.629393	-2.053722	1.801728	0.008015	0.703011
-42.887210	-2.009650	1.806733	0.008063	0.703007
-42.908297	-2.007401	1.811738	0.008067	0.703004
-42.562759	-2.066617	1.816742	0.008003	0.703009
-42.759480	-2.036260	1.821747	0.008039	0.703000
-42.778830	-2.027557	1.826752	0.008043	0.703010
-42.939490	-2.127847	1.831757	0.008073	0.702750
-43.909013	-1.983103	1.836762	0.008253	0.702693
-43.889955	-1.984419	1.841766	0.008249	0.702698
-43.805010	-2.003932	1.846771	0.008233	0.702689
-43.268122	-2.095029	1.851776	0.008133	0.702699
-43.540658	-2.049528	1.856781	0.008184	0.702693
-44.133710	-1.942630	1.861786	0.008294	0.702695
-43.632886	-2.108056	1.866790	0.008201	0.702541
-44.525536	-2.034499	1.871795	0.008367	0.702369
-44.418716	-2.049225	1.876800	0.008347	0.702377
-44.668099	-2.008429	1.881805	0.008394	0.702370
-44.497710	-2.038544	1.886810	0.008362	0.702371
-44.381916	-2.055449	1.891814	0.008340	0.702379
-44.734441	-1.998733	1.896819	0.008406	0.702366
-44.717183	-2.074272	1.901824	0.008402	0.702220
-45.420068	-2.019804	1.906829	0.008533	0.702077
-45.382513	-2.026157	1.911834	0.008526	0.702078
-45.281870	-2.041404	1.916838	0.008507	0.702083
-45.360265	-2.032677	1.921843	0.008522	0.702073
-45.329645	-2.032815	1.926848	0.008516	0.702084
-45.202613	-2.058479	1.931853	0.008492	0.702078
-45.463418	-2.127461	1.936858	0.008541	0.701844
-46.488869	-1.990787	1.941862	0.008732	0.701751
-46.580781	-1.978798	1.946867	0.008749	0.701742
-46.046686	-2.069255	1.951872	0.008649	0.701752
-46.159988	-2.051948	1.956877	0.008670	0.701747
-46.439033	-2.002811	1.961882	0.008722	0.701745
-46.324944	-2.019030	1.966886	0.008701	0.701754
-46.360513	-2.093182	1.971891	0.008707	0.701591
-47.250270	-2.007210	1.976896	0.008873	0.701444
-47.359289	-1.991628	1.981901	0.008893	0.701437
-47.418778	-1.982257	1.986906	0.008904	0.701434
-47.115076	-2.031983	1.991910	0.008847	0.701443
-47.176112	-2.026037	1.996915	0.008859	0.701434
-47.079567	-2.045649	2.001920	0.008841	0.701429

-47.689060	-2.085984	2.011917	0.008954	0.701127
-47.900990	-2.050398	2.021914	0.008993	0.701123
-48.088443	-2.017363	2.031910	0.009028	0.701123
-47.850643	-2.059620	2.041907	0.008983	0.701123
-47.812735	-2.065113	2.051904	0.008976	0.701126
-47.914053	-2.047708	2.061901	0.008995	0.701125
-47.756122	-2.075298	2.071898	0.008965	0.701127
-48.058574	-2.022026	2.081894	0.009021	0.701126
-48.009172	-2.032501	2.091891	0.009012	0.701123
-47.904153	-2.050000	2.101888	0.008992	0.701126
-47.416710	-2.034428	2.111885	0.008901	0.701333
-47.136694	-2.032642	2.121882	0.008849	0.701439
-47.035592	-2.051410	2.131878	0.008830	0.701437
-47.037498	-2.050961	2.141875	0.008830	0.701438
-47.103262	-2.038391	2.151872	0.008842	0.701440
-47.064250	-2.045083	2.161869	0.008835	0.701441
-46.525287	-2.049577	2.171866	0.008734	0.701627
-46.340006	-2.023807	2.181862	0.008700	0.701746
-46.142651	-2.058000	2.191859	0.008663	0.701748
-46.087124	-2.067483	2.201856	0.008652	0.701749
-46.403344	-1.989010	2.211853	0.008711	0.701794
-45.406341	-2.028685	2.221850	0.008525	0.702074
-45.296817	-2.049727	2.231846	0.008505	0.702071
-45.357140	-2.036504	2.241843	0.008516	0.702077
-45.414702	-1.985826	2.251840	0.008526	0.702159
-44.484587	-2.046007	2.261837	0.008353	0.702373
-44.547471	-2.035574	2.271834	0.008365	0.702371
-44.611457	-2.025021	2.281830	0.008376	0.702370
-44.203707	-2.014260	2.291827	0.008300	0.702539
-43.680334	-2.030282	2.301824	0.008203	0.702696
-43.986036	-1.975857	2.311821	0.008259	0.702696
-43.660425	-2.024909	2.321818	0.008199	0.702714
-43.040294	-1.991614	2.331814	0.008083	0.703005
-42.759942	-2.041878	2.341811	0.008031	0.703005
-42.873628	-2.020723	2.351808	0.008051	0.703007
-42.546707	-1.991404	2.361805	0.007990	0.703184
-41.970435	-2.016585	2.371802	0.007883	0.703341
-41.649372	-2.075926	2.381798	0.007823	0.703337
-41.917354	-2.026797	2.391795	0.007873	0.703340
-41.272104	-2.017748	2.401792	0.007752	0.703591
-41.370617	-1.977301	2.411789	0.007771	0.703638
-41.095436	-2.027415	2.421786	0.007719	0.703636
-40.864577	-1.994985	2.431782	0.007676	0.703785
-40.053840	-2.057012	2.441779	0.007525	0.703952
-40.391105	-1.995299	2.451776	0.007588	0.703955
-40.249557	-2.020774	2.461773	0.007561	0.703955
-39.723767	-1.964685	2.471770	0.007463	0.704257
-39.279464	-2.042391	2.481766	0.007380	0.704261
-39.295192	-2.038972	2.491763	0.007383	0.704262
-39.230067	-1.962151	2.501760	0.007371	0.704441
-38.563571	-2.005862	2.511757	0.007246	0.704592
-38.517424	-2.014715	2.521754	0.007238	0.704592
-38.689262	-1.956470	2.531750	0.007269	0.704648
-37.435782	-2.061112	2.541747	0.007036	0.704887
-37.746106	-2.004436	2.551744	0.007093	0.704890
-37.531667	-2.043602	2.561741	0.007053	0.704889
-37.408353	-1.957355	2.571738	0.007030	0.705107
-36.694142	-2.032824	2.581734	0.006897	0.705212
-36.889122	-1.998458	2.591731	0.006933	0.705211
-36.677980	-1.995805	2.601728	0.006894	0.705293
-36.023311	-1.996527	2.611725	0.006772	0.705526
-35.818574	-2.033923	2.621722	0.006733	0.705525
-35.988433	-2.004308	2.631718	0.006765	0.705524
-35.232176	-2.008488	2.641715	0.006624	0.705787
-35.043831	-2.004650	2.651712	0.006589	0.705863
-34.846853	-2.039964	2.661709	0.006552	0.705863
-35.078204	-1.979842	2.671706	0.006595	0.705901
-34.300289	-2.006660	2.681702	0.006450	0.706126
-34.157408	-2.031397	2.691699	0.006423	0.706128
-34.191298	-2.025244	2.701696	0.006429	0.706128
-33.609147	-2.011021	2.711693	0.006320	0.706366
-33.509417	-1.990108	2.721690	0.006302	0.706444
-33.230427	-2.041400	2.731686	0.006250	0.706441
-33.172686	-2.000591	2.741683	0.006239	0.706544
-32.511704	-2.015557	2.751680	0.006115	0.706751
-32.168384	-2.077266	2.761677	0.006051	0.706750
-32.479428	-2.022021	2.771674	0.006109	0.706750
-31.758321	-2.020697	2.781670	0.005975	0.707011
-31.616854	-2.011507	2.791667	0.005948	0.707081
-31.484715	-2.035338	2.801664	0.005923	0.707081
-31.525080	-1.984507	2.811661	0.005931	0.707168
-30.779281	-2.016127	2.821658	0.005792	0.707372
-30.706137	-2.027183	2.831654	0.005778	0.707376
-30.881172	-1.996300	2.841651	0.005810	0.707376
-30.121490	-1.975505	2.851648	0.005669	0.707690
-29.845980	-2.021188	2.861645	0.005617	0.707697
-29.880684	-2.015592	2.871642	0.005623	0.707696
-29.456186	-2.003267	2.881638	0.005544	0.707873
-28.933251	-2.029163	2.891635	0.005447	0.708008
-28.864298	-2.039820	2.901632	0.005434	0.708012
-29.095630	-1.993058	2.911629	0.005477	0.708023
-28.285723	-1.976261	2.921626	0.005326	0.708347
-28.022072	-2.022048	2.931622	0.005276	0.708349
-28.097369	-2.009256	2.941619	0.005290	0.708348
-27.646538	-2.016477	2.951616	0.005206	0.708495
-27.068511	-2.047717	2.961613	0.005098	0.708639
-27.203016	-2.024529	2.971610	0.005123	0.708638
-27.308384	-2.007276	2.981606	0.005143	0.708635
-26.621268	-1.973673	2.991603	0.005015	0.708948
-26.456088	-1.999214	3.001600	0.004984	0.708956
-26.505604	-1.992306	3.011597	0.004993	0.708953
-25.908768	-1.993461	3.021594	0.004881	0.709164
-25.518161	-2.015125	3.031590	0.004808	0.709260
-25.480849	-2.020686	3.041587	0.004801	0.709262
-25.341113	-2.022981	3.051584	0.004775	0.709308
-24.929687	-1.953994	3.061581	0.004698	0.709593
-24.570176	-2.017601	3.071578	0.004631	0.709594
-24.783790	-1.980473	3.081574	0.004671	0.709593
-24.160918	-1.976080	3.091571	0.004555	0.709824
-23.814917	-2.004013	3.101568	0.004490	0.709892
-23.806054	-2.006496	3.111565	0.004488	0.709890
-23.601077	-1.988885	3.121562	0.004450	0.709999
-22.775164	-2.028581	3.131558	0.004296	0.710214
-22.727428	-2.036897	3.141555	0.004287	0.710214
-22.543043	-2.069838	3.151552	0.004253	0.710215
-22.703582	-1.942389	3.161549	0.004282	0.710412
-21.736310	-2.056629	3.171546	0.004102	0.710529
-22.059205	-1.999170	3.181542	0.004162	0.710529
-21.921694	-2.004623	3.191539	0.004136	0.710567
-21.150085	-1.990782	3.201536	0.003992	0.710870
-20.722504	-2.066003	3.211533	0.003913	0.710872
-20.906704	-2.035062	3.221530	0.003947	0.710869
-20.994836	-1.962671	3.231526	0.003963	0.710982
-20.288133	-2.012015	3.241523	0.003831	0.711135
-20.139546	-2.038928	3.251520	0.003803	0.711135
-20.434909	-1.968949	3.261517	0.003858	0.711170
-19.419003	-2.009354	3.271514	0.003669	0.711451
-19.328067	-2.025954	3.281510	0.003652	0.711450
-19.172915	-2.052156	3.291507	0.003623	0.711453
-19.114611	-1.968110	3.301504	0.003612	0.711642
-18.609016	-1.999022	3.311501	0.003517	0.711760
-18.682652	-1.986061	3.321498	0.003531	0.711760
-18.458258	-1.981046	3.331494	0.003489	0.711850
-17.609328	-2.013001	3.341491	0.003331	0.712088
-17.433036	-2.043084	3.351488	0.003298	0.712091
-17.655784	-2.004378	3.361485	0.003339	0.712090
-17.022506	-2.000216	3.371482	0.003221	0.712323
-17.023621	-1.969105	3.381478	0.003221	0.712385
-16.595935	-2.047120	3.391475	0.003141	0.712382
-16.833651	-1.946381	3.401472	0.003185	0.712498
-15.709756	-2.039769	3.411469	0.002976	0.712712
-16.006251	-1.989692	3.421466	0.003031	0.712706
-15.976622	-1.993640	3.431462	0.003025	0.712709
-15.231001	-1.983623	3.441459	0.002886	0.712994
-15.134515	-1.986720	3.451456	0.002868	0.713022
-14.809513	-2.045062	3.461453	0.002807	0.713022
-14.828435	-1.974926	3.471450	0.002811	0.713155
-14.205104	-1.984831	3.481446	0.002694	0.713357
-13.805699	-2.055722	3.491443	0.002620	0.713357
-14.206642	-1.983032	3.501440	0.002694	0.713360
-13.460465	-2.000485	3.511437	0.002555	0.713590
-13.227488	-2.012400	3.521434	0.002512	0.713649
-12.957653	-2.059417	3.531430	0.002461	0.713652
-13.162440	-2.003909	3.541427	0.002499	0.713690
-12.370781	-2.003373	3.551424	0.002352	0.713972
-12.092286	-2.054174	3.561421	0.002300	0.713970
-12.480913	-1.985882	3.571418	0.002372	0.713968
-12.118048	-1.958105	3.581414	0.002304	0.714152
-11.429479	-2.019138	3.591411	0.002176	0.714275
-11.531738	-1.998562	3.601408	0.002195	0.714280
-11.417456	-1.980209	3.611405	0.002173	0.714357
-10.727489	-1.978258	3.621402	0.002045	0.714605
-10.691877	-1.985275	3.631398	0.002038	0.714604
-10.650776	-1.991538	3.641395	0.002030	0.714607
-9.966756	-1.988677	3.651392	0.001902	0.714855
-9.764685	-1.998413	3.661389	0.001865	0.714907
-9.810847	-1.991413	3.671386	0.001873	0.714905
-9.735202	-1.951607	3.681382	0.001859	0.715011
-8.761972	-2.015439	3.691379	0.001677	0.715229
-8.883923	-1.993874	3.701376	0.001700	0.715229
-8.948827	-1.982433	3.711373	0.001712	0.715229
-8.208625	-1.969833	3.721370	0.001574	0.715516
-7.975041	-1.997849	3.731366	0.001530	0.715543
-7.817831	-2.024084	3.741363	0.001501	0.715547
-7.921644	-1.947921	3.751360	0.001520	0.715661
-6.820189	-2.031169	3.761357	0.001315	0.715886
-7.165094	-1.970796	3.771354	0.001379	0.715884
-6.869843	-2.025327	3.781350	0.001324	0.715880
-6.566070	-1.996537	3.791347	0.001267	0.716045
-6.101255	-2.034526	3.801344	0.001180	0.716134
-6.326917	-1.994252	3.811341	0.001222	0.716134
-6.240051	-1.983611	3.821338	0.001206	0.716186
-5.784698	-1.932294	3.831334	0.001121	0.716449
-5.888164	-1.913629	3.841331	0.001140	0.716450
-5.410238	-1.974136	3.851328	0.001051	0.716499
-4.464338	-2.012743	3.861325	0.000874	0.716756
-4.843959	-1.947454	3.871322	0.000945	0.716752
-4.364929	-2.032311	3.881318	0.000856	0.716753
-4.315349	-1.932026	3.891315	0.000846	0.716970
-3.830855	-1.959865	3.901312	0.000756	0.717085
-3.704823	-1.982317	3.911309	0.000732	0.717086
-4.835787	-1.700624	3.921306	0.000942	0.717245
-2.528033	-2.043634	3.931302	0.000513	0.717380
-3.379985	-1.890306	3.941299	0.000671	0.717383
-3.311448	-1.815240	3.951296	0.000658	0.717556
-2.256764	-1.925646	3.961293	0.000462	0.717709
-2.566114	-1.872288	3.971290	0.000519	0.717706
-2.423347	-1.833498	3.981286	0.000492	0.717834
-2.129787	-1.792401	3.991283	0.000437	0.718018
-3.217219	-1.590411	4.001280	0.000640	0.718035
-2.050050	-1.636543	4.011277	0.000422	0.718355
-1.876608	-1.668268	4.021274	0.000390	0.718354
-0.969508	-1.748132	4.031270	0.000221	0.718515
-1.188765	-1.642610	4.041267	0.000261	0.718647
-1.628780	-1.545476	4.051264	0.000343	0.718684
-1.536932	-1.420807	4.061261	0.000326	0.718963
-1.816958	-1.334611	4.071258	0.000377	0.719035
-1.857632	-1.207909	4.081254	0.000385	0.719271
-1.204210	-1.226744	4.091251	0.000263	0.719463
-0.900303	-1.208401	4.101248	0.000206	0.719606
-0.554189	-1.157941	4.111245	0.000142	0.719828
-1.266068	-0.977700	4.121242	0.000274	0.719933
-0.747739	-0.922900	4.131238	0.000177	0.720223
-0.877987	-0.809260	4.141235	0.000201	0.720402
-1.035460	-0.687853	4.151232	0.000230	0.720586
-0.555489	-0.623343	4.161229	0.000141	0.720881
-0.394887	-0.563441	4.171226	0.000110	0.721056
-0.263665	-0.502298	4.181222	0.000086	0.721222
-0.377467	-0.366699	4.191219	0.000107	0.721449
-0.594376	-0.176162	4.201216	0.000147	0.721748
0.056189	-0.153672	4.211213	0.000026	0.722020
-0.405930	0.046583	4.221210	0.000111	0.722253
0.000000	0.129647	4.231206	0.000035	0.722558

0.136457	0.749274	4.236211	0.000010	0.723821
0.362076	1.978392	4.241216	-0.000033	0.726304
0.904012	3.743958	4.246221	-0.000135	0.729931
1.770010	6.016447	4.251226	-0.000298	0.734632
2.400652	8.839857	4.256230	-0.000418	0.740278
3.520837	12.069068	4.261235	-0.000628	0.746817
5.173152	15.679153	4.266240	-0.000938	0.754194
7.202198	19.634030	4.271245	-0.001319	0.762266
10.204865	23.859556	4.276250	-0.001881	0.771068
13.972545	28.366025	4.281254	-0.002585	0.780526
17.140720	33.386676	4.286259	-0.003179	0.790601
18.843371	38.972138	4.291264	-0.003499	0.801089
20.549413	44.866134	4.296269	-0.003821	0.811980
21.813930	51.136690	4.301274	-0.004061	0.823241
22.534661	57.777525	4.306278	-0.004199	0.834814
23.571448	64.553627	4.311283	-0.004397	0.846549
24.388822	71.596579	4.316288	-0.004554	0.858500
24.909040	78.879839	4.321293	-0.004655	0.870592
25.980698	86.244025	4.326298	-0.004860	0.882804
27.216731	93.759663	4.331302	-0.005095	0.895134
28.234588	101.468898	4.336307	-0.005290	0.907539
28.967441	109.372464	4.341312	-0.005431	0.919998
30.014626	117.319869	4.346317	-0.005632	0.932440
31.145252	125.369202	4.351322	-0.005847	0.944893
31.705237	133.612974	4.356326	-0.005957	0.957324
32.251719	141.934452	4.361331	-0.006064	0.969704
33.185121	150.268326	4.366336	-0.006244	0.982044
33.907833	158.722675	4.371341	-0.006384	0.994349
34.652894	167.189602	4.376346	-0.006528	1.006527
35.185164	175.735501	4.381350	-0.006633	1.018617
35.744411	184.313744	4.386355	-0.006743	1.030616
36.363131	192.903077	4.391360	-0.006864	1.042506
37.159793	201.489870	4.396365	-0.007018	1.054299
37.570660	210.167792	4.401370	-0.007100	1.065993
38.071259	218.841987	4.406374	-0.007199	1.077576
38.706824	227.477560	4.411379	-0.007323	1.089016
39.622381	236.093059	4.416384	-0.007499	1.100372
40.217516	244.762744	4.421389	-0.007616	1.111611
40.763571	253.441331	4.426394	-0.007723	1.122737
41.410187	262.093851	4.431398	-0.007849	1.133743
42.024552	270.748702	4.436403	-0.007969	1.144639
42.508056	279.460809	4.441408	-0.008065	1.155475
43.220201	288.050593	4.446413	-0.008203	1.166108
43.792467	296.681302	4.451418	-0.008316	1.176666
44.209155	305.308183	4.456422	-0.008399	1.187093
44.994952	313.875048	4.461427	-0.008551	1.197432
45.795256	322.427087	4.466432	-0.008706	1.207668
46.493710	330.988610	4.471437	-0.008841	1.217809
46.803373	339.614983	4.476442	-0.008905	1.227864
47.531681	348.159536	4.481446	-0.009046	1.237825
48.435011	356.635379	4.486451	-0.009220	1.247661
48.946843	365.192611	4.491456	-0.009321	1.257438
49.384325	373.716851	4.496461	-0.009408	1.267087
50.258312	382.190075	4.501466	-0.009576	1.276689
50.857220	390.664249	4.506470	-0.009693	1.286169
51.013511	399.228177	4.511475	-0.009728	1.295595
51.566699	407.696913	4.516480	-0.009837	1.304923
52.132748	416.259767	4.521485	-0.009948	1.314288
52.755970	424.682086	4.526490	-0.010069	1.323446
53.291539	433.098376	4.531494	-0.010175	1.332519
53.828249	441.491212	4.536499	-0.010280	1.341506
54.325292	449.911087	4.541504	-0.010378	1.350454
54.728069	458.310395	4.546509	-0.010459	1.359305
55.386170	466.665364	4.551514	-0.010587	1.368097
55.902508	475.040199	4.556518	-0.010689	1.376828
56.470813	483.387307	4.561523	-0.010800	1.385485
57.110416	491.758681	4.566528	-0.010924	1.394125
57.548925	500.107371	4.571533	-0.011012	1.402654
58.164061	508.439959	4.576538	-0.011132	1.411145
58.574695	516.790562	4.581542	-0.011214	1.419569
58.960761	525.136487	4.586547	-0.011291	1.427935
59.536332	533.460209	4.591552	-0.011404	1.436260
59.965108	541.769733	4.596557	-0.011489	1.444500
60.540418	550.090621	4.601562	-0.011602	1.452728
60.840740	558.409415	4.606566	-0.011663	1.460863
61.133558	566.746673	4.611571	-0.011723	1.468969
61.719453	575.064344	4.616576	-0.011838	1.477058
62.051397	583.330580	4.621581	-0.011905	1.485014
62.490325	591.614784	4.626586	-0.011992	1.492961
62.598435	599.921045	4.631590	-0.012018	1.500836
63.135493	608.161096	4.636595	-0.012123	1.508673
63.583504	616.434348	4.641600	-0.012212	1.516487
63.829651	624.698234	4.646605	-0.012264	1.524222
64.233513	632.959928	4.651610	-0.012344	1.531939
64.636938	641.200445	4.656614	-0.012425	1.539597
65.086027	649.440870	4.661619	-0.012514	1.547224
65.711577	657.684396	4.666624	-0.012636	1.554843
65.975372	665.915380	4.671629	-0.012690	1.562360
66.267158	674.173036	4.676634	-0.012750	1.569868
66.501746	682.436568	4.681638	-0.012799	1.577338
66.810647	690.658452	4.686643	-0.012862	1.584746
67.319036	698.872731	4.691648	-0.012962	1.592141
67.362461	707.124936	4.696653	-0.012976	1.599470
67.751417	715.328452	4.701658	-0.013054	1.606771
68.121234	723.545088	4.706662	-0.013128	1.614047
68.291959	731.766990	4.711667	-0.013165	1.621267
68.772941	739.961449	4.716672	-0.013260	1.628475
69.022540	748.221468	4.721677	-0.013312	1.635675
69.356115	756.390530	4.726682	-0.013380	1.642777
69.587938	764.577557	4.731686	-0.013428	1.649850
70.219742	772.722116	4.736691	-0.013551	1.656911
70.563565	780.912514	4.741696	-0.013621	1.663941
70.762211	789.117354	4.746701	-0.013663	1.670935
71.013026	797.321732	4.751706	-0.013715	1.677905
71.367217	805.478227	4.756710	-0.013787	1.684821
71.737631	813.655455	4.761715	-0.013861	1.691727
71.958489	821.868992	4.766720	-0.013908	1.698616
72.218963	830.023399	4.771725	-0.013962	1.705433
72.535288	838.236874	4.776730	-0.014026	1.712279
73.405958	846.313339	4.781734	-0.014193	1.719057
74.433473	854.370556	4.786739	-0.014390	1.725812
74.727092	862.596631	4.791744	-0.014450	1.732584
74.698812	870.828592	4.796749	-0.014450	1.739293
75.093655	878.979710	4.801754	-0.014529	1.745965
75.318985	887.178897	4.806758	-0.014577	1.752629
75.484801	895.356574	4.811763	-0.014613	1.759243
75.668040	903.522981	4.816768	-0.014652	1.765825
75.953493	911.679333	4.821773	-0.014711	1.772387
76.253686	919.850008	4.826778	-0.014772	1.778938
76.474965	928.001174	4.831782	-0.014819	1.785440
76.862350	936.183796	4.836787	-0.014896	1.791963
77.362069	944.328266	4.841792	-0.014995	1.798446
77.203739	952.491437	4.846797	-0.014971	1.804841
77.660467	960.616929	4.851802	-0.015061	1.811257
77.771696	968.789962	4.856806	-0.015087	1.817647
77.823689	976.935451	4.861811	-0.015102	1.823985
78.147698	985.075341	4.866816	-0.015168	1.830330
78.543811	993.183703	4.871821	-0.015247	1.836637
78.783132	1001.324500	4.876826	-0.015297	1.842929
79.236713	1009.434193	4.881830	-0.015387	1.849200
79.264362	1017.611130	4.886835	-0.015398	1.855452
79.809162	1025.701261	4.891840	-0.015504	1.861677
79.829388	1033.865986	4.896845	-0.015514	1.867876
80.183984	1042.026286	4.901850	-0.015585	1.874091
80.411093	1050.139929	4.906854	-0.015633	1.880235
80.500585	1058.256561	4.911859	-0.015655	1.886345
80.733861	1066.410320	4.916864	-0.015704	1.892480
81.102619	1074.504873	4.921869	-0.015778	1.898566
81.437539	1082.615129	4.926874	-0.015845	1.904640
81.415821	1090.785582	4.931878	-0.015847	1.910700
81.500370	1098.920247	4.936883	-0.015868	1.916725
81.832946	1107.022793	4.941888	-0.015935	1.922736
82.099761	1115.124551	4.946893	-0.015990	1.928720
82.465015	1123.247140	4.951898	-0.016064	1.934712
82.547840	1131.376737	4.956902	-0.016084	1.940659
82.799389	1139.490988	4.961907	-0.016137	1.946595
83.101232	1147.650697	4.966912	-0.016198	1.952552
83.315493	1155.742884	4.971917	-0.016243	1.958432
83.588597	1163.825657	4.976922	-0.016300	1.964293
83.620142	1171.952199	4.981926	-0.016311	1.970143
83.768153	1180.074881	4.986931	-0.016344	1.975985
84.196893	1188.152359	4.991936	-0.016429	1.981808
84.348672	1196.257495	4.996941	-0.016463	1.987604
84.642203	1204.368440	5.001946	-0.016523	1.993402
84.837468	1212.474634	5.006950	-0.016564	1.999169
85.159439	1220.543834	5.011955	-0.016630	2.004907
85.321939	1228.684889	5.016960	-0.016665	2.010662
85.628759	1236.782709	5.021965	-0.016728	2.016385
85.917411	1244.873035	5.026970	-0.016787	2.022085
86.571117	1252.927677	5.031974	-0.016914	2.027782
86.636286	1261.092437	5.036979	-0.016931	2.033479
87.174363	1269.160888	5.041984	-0.017037	2.039141
87.370485	1277.239297	5.046989	-0.017079	2.044759
87.599912	1285.364167	5.051994	-0.017127	2.050398
87.747077	1293.487143	5.056998	-0.017160	2.056011
88.063364	1301.552446	5.062003	-0.017224	2.061587
88.279972	1309.674028	5.067008	-0.017270	2.067175
88.265670	1317.817636	5.072013	-0.017272	2.072741
88.749784	1325.867863	5.077018	-0.017368	2.078278
89.071107	1333.944337	5.082022	-0.017433	2.083802
89.319829	1342.048913	5.087027	-0.017485	2.089322
89.577149	1350.168806	5.092032	-0.017538	2.094840
89.564425	1358.280649	5.097037	-0.017541	2.100311
89.709353	1366.374571	5.102042	-0.017573	2.105771
90.043124	1374.506352	5.107046	-0.017641	2.111260
90.305401	1382.609647	5.112051	-0.017695	2.116710
90.341372	1390.695730	5.117056	-0.017707	2.122112
90.804763	1398.719569	5.122061	-0.017799	2.127499
91.173949	1406.813662	5.127066	-0.017873	2.132911
91.377329	1414.906648	5.132070	-0.017916	2.138292
91.607444	1422.971662	5.137075	-0.017964	2.143644
92.070331	1431.042185	5.142080	-0.018056	2.149008
92.291221	1439.155003	5.147085	-0.018102	2.154364
92.555538	1447.231239	5.152090	-0.018157	2.159686
92.841990	1455.296986	5.157094	-0.018216	2.164991
93.067095	1463.374956	5.162099	-0.018263	2.170285
93.224775	1471.504503	5.167104	-0.018298	2.175593
93.348404	1479.578026	5.172109	-0.018326	2.180848
93.525606	1487.666910	5.177114	-0.018364	2.186106
93.727366	1495.784992	5.182118	-0.018407	2.191372
94.027449	1503.854088	5.187123	-0.018468	2.196603
94.310732	1511.917575	5.192128	-0.018527	2.201816
94.362219	1519.990468	5.197133	-0.018541	2.207002
94.669294	1528.067887	5.202138	-0.018604	2.212202
95.062385	1536.130187	5.207142	-0.018683	2.217387
95.320999	1544.189345	5.212147	-0.018736	2.222547
95.648128	1552.281910	5.217152	-0.018802	2.227721
95.758563	1560.380527	5.222157	-0.018828	2.232868
96.017402	1568.466798	5.227162	-0.018882	2.238009
96.305955	1576.523656	5.232166	-0.018941	2.243122
96.532459	1584.587426	5.237171	-0.018988	2.248222
96.841047	1592.689080	5.242176	-0.019051	2.253341
97.036413	1600.760843	5.247181	-0.019093	2.258420
97.022671	1608.869728	5.252186	-0.019096	2.263493
97.259020	1616.942601	5.257190	-0.019145	2.268553
97.509867	1625.074070	5.262195	-0.019197	2.273640
97.604568	1633.162055	5.267200	-0.019220	2.278675
97.757580	1641.190154	5.272205	-0.019254	2.283667
98.227657	1649.203076	5.277210	-0.019347	2.288665
98.418768	1657.298590	5.282214	-0.019388	2.293680
98.747100	1665.335519	5.287219	-0.019454	2.298659
99.248492	1673.378299	5.292224	-0.019553	2.303646
99.694729	1681.419169	5.297229	-0.019641	2.308616
99.877364	1689.533435	5.302234	-0.019681	2.313598
100.310398	1697.581715	5.307238	-0.019767	2.318549
100.647742	1705.620832	5.312243	-0.019835	2.323477
100.907218	1713.717936	5.317248	-0.019888	2.328423
100.913084	1721.830920	5.322253	-0.019895	2.333347
101.229188	1729.896179	5.327258	-0.019959	2.338257
101.456238	1737.957350	5.332262	-0.020007	2.343147
101.552612	1746.051943	5.337267	-0.020030	2.348037
101.928605	1754.143297	5.342272	-0.020105	2.352937
102.149587	1762.192331	5.347277	-0.020152	2.357788
102.395211	1770.231312	5.352282	-0.020203	2.362626
102.572468	1778.310268	5.357286	-0.020241	2.367472
102.767558	1786.374709	5.362291	-0.020283	2.372301
103.059297	1794.453230	5.367296	-0.020343	2.377136
103.099245	1802.508848	5.372301	-0.020355	2.381928
103.654933	1810.555087	5.377306	-0.020464	2.386746
103.863071	1818.647304	5.382310	-0.020508	2.391553
103.823920	1826.730804	5.387315	-0.020506	2.396326
104.376333	1834.753086	5.392320	-0.020615	2.401100
104.429994	1842.826011	5.397325	-0.020630	2.405855
104.821723	1850.871586	5.402330	-0.020708	2.410610
105.276061	1858.940731	5.407334	-0.020798	2.415376
105.411976	1867.001302	5.412339	-0.020829	2.420101
105.729086	1875.063371	5.417344	-0.020893	2.424833
105.990702	1883.110395	5.422349	-0.020947	2.429542
106.242907	1891.269567	5.427354	-0.020999	2.434307
106.809719	1899.272056	5.432358	-0.021110	2.438995
106.802070	1907.326288	5.437363	-0.021114	2.443660
106.893742	1915.416912	5.442368	-0.021137	2.448345
107.048134	1923.475343	5.447373	-0.021171	2.453008
107.483718	1931.498802	5.452378	-0.021257	2.457662
107.600447	1939.565349	5.457382	-0.021284	2.462308
107.987484	1947.585489	5.462387	-0.021362	2.466940
108.526574	1955.654591	5.467392	-0.021467	2.471601
108.624483	1963.735527	5.472397	-0.021491	2.476228
108.794141	1971.797946	5.477402	-0.021528	2.480841
109.228589	1979.829577	5.482406	-0.021614	2.485448
109.391583	1987.889332	5.487411	-0.021650	2.490041
109.750855	1995.967582	5.492416	-0.021722	2.494651
109.736439	2004.031253	5.497421	-0.021725	2.499217
110.004957	2012.075082	5.502426	-0.021780	2.503784
109.958170	2020.186600	5.507430	-0.021777	2.508358
110.280155	2028.259342	5.512435	-0.021842	2.512929
110.457527	2036.316666	5.517440	-0.021880	2.517472
110.528231	2044.348065	5.522445	-0.021899	2.521984
110.656818	2052.395412	5.527450	-0.021928	2.526502
111.028931	2060.435039	5.532454	-0.022003	2.531024
111.068548	2068.516081	5.537459	-0.022015	2.535538
111.195006	2076.569079	5.542464	-0.022044	2.540034
111.653306	2084.561877	5.547469	-0.022135	2.544513
112.050875	2092.615318	5.552474	-0.022214	2.549012
112.194448	2100.722254	5.557478	-0.022246	2.553516
112.387170	2108.750114	5.562483	-0.022288	2.557971
112.860546	2116.788262	5.567488	-0.022381	2.562444
113.160538	2124.815905	5.572493	-0.022442	2.566891
113.516871	2132.895689	5.577498	-0.022514	2.571363
113.832941	2140.966687	5.582502	-0.022578	2.575819
114.019365	2149.016610	5.587507	-0.022618	2.580247
114.048745	2157.084512	5.592512	-0.022629	2.584667
114.197071	2165.154481	5.597517	-0.022662	2.589088
114.414375	2173.393486	5.602522	-0.022708	2.593598
114.739195	2181.400927	5.607526	-0.022774	2.597982
114.889735	2189.396154	5.612531	-0.022807	2.602340
115.086332	2197.406050	5.617536	-0.022849	2.606702
115.337027	2205.442650	5.622541	-0.022901	2.611075
115.662134	2213.473242	5.627546	-0.022967	2.615441
116.059605	2221.506172	5.632550	-0.023046	2.619807
116.032736	2229.551691	5.637555	-0.023046	2.624144
116.237472	2237.605387	5.642560	-0.023090	2.628493
116.308312	2245.680359	5.647565	-0.023108	2.632838
116.822682	2253.671554	5.652570	-0.023209	2.637160
117.129426	2261.723883	5.657574	-0.023272	2.641494
116.922650	2269.804218	5.662579	-0.023239	2.645802
117.247596	2277.846731	5.667584	-0.023305	2.650117
117.618955	2285.866392	5.672589	-0.023379	2.654417
117.903889	2293.899868	5.677594	-0.023437	2.658711
118.359892	2301.942681	5.682598	-0.023528	2.663014
118.745033	2309.957939	5.687603	-0.023605	2.667290
119.099676	2318.049003	5.692608	-0.023676	2.671598
119.181618	2326.136834	5.697613	-0.023697	2.675880
119.329091	2334.158706	5.702618	-0.023729	2.680125
119.611846	2342.193607	5.707622	-0.023787	2.684378
119.663296	2350.258106	5.712627	-0.023802	2.688625
120.025639	2358.305008	5.717632	-0.023875	2.692876
120.132987	2366.361026	5.722637	-0.023900	2.697109
120.340744	2374.397407	5.727642	-0.023944	2.701331
120.489036	2382.469766	5.732646	-0.023977	2.705562
120.723199	2390.487706	5.737651	-0.024026	2.709762
120.957133	2398.563811	5.742656	-0.024075	2.713987
121.182174	2406.587074	5.747661	-0.024122	2.718177
121.506417	2414.621238	5.752666	-0.024188	2.722373
121.715368	2422.664263	5.757670	-0.024232	2.726559
121.675600	2430.742726	5.762675	-0.024230	2.730742
122.016631	2438.808276	5.767680	-0.024299	2.734935
122.416113	2446.790554	5.772685	-0.024379	2.739082
122.364570	2454.853693	5.777690	-0.024374	2.743237
122.699979	2462.897269	5.782694	-0.024442	2.747399
122.891204	2470.978759	5.787699	-0.024483	2.751566
123.258696	2479.073769	5.792704	-0.024557	2.755744
123.610940	2487.067870	5.797709	-0.024628	2.759863
123.915380	2495.071186	5.802714	-0.024690	2.763977
124.199812	2503.109739	5.807718	-0.024748	2.768102
124.276577	2511.160867	5.812723	-0.024768	2.772215
124.472205	2519.245686	5.817728	-0.024810	2.776346
124.624627	2527.279538	5.822733	-0.024843	2.780443
124.676129	2535.303253	5.827738	-0.024858	2.784522
124.908339	2543.366428	5.832742	-0.024907	2.788626
125.108999	2551.413206	5.837747	-0.024949	2.792713
125.325631	2559.458924	5.842752	-0.024995	2.796795
125.349833	2567.501659	5.847757	-0.025005	2.800859
125.592786	2575.504823	5.852762	-0.025055	2.804909
126.118103	2583.538036	5.857766	-0.025159	2.808985
126.135820	2591.592526	5.862771	-0.025167	2.813036
126.695722	2599.628734	5.867776	-0.025277	2.817103
126.902711	2607.678703	5.872781	-0.025321	2.821151
127.132364	2615.705313	5.877786	-0.025369	2.825183
127.240108	2623.783076	5.882790	-0.025394	2.829227
127.398036	2631.860483	5.887795	-0.025429	2.833269
127.877272	2639.882223	5.892800	-0.025523	2.837295
128.151048	2647.888777	5.897805	-0.025580	2.841296
128.395273	2655.902586	5.902810	-0.025631	2.845294
128.638357	2663.946818	5.907814	-0.025681	2.849300
128.614280	2672.022012	5.912819	-0.025682	2.853302
128.932558	2680.064839	5.917824	-0.025747	2.857301
129.238670	2688.069291	5.922829	-0.025809	2.861275
129.354130	2696.105862	5.927834	-0.025836	2.865248
129.585796	2704.174834	5.932838	-0.025884	2.869238
129.685982	2712.233736	5.937843	-0.025908	2.873211
129.976769	2720.279345	5.942848	-0.025968	2.877181
129.973192	2728.324570	5.947853	-0.025972	2.881130
130.328969	2736.301248	5.952858	-0.026044	2.885060
130.772952	2744.338533	5.957862	-0.026132	2.889019
130.915050	2752.410417	5.962867	-0.026164	2.892973
131.178322	2760.461427	5.967872	-0.026218	2.896917
131.541516	2768.478530	5.972877	-0.026291	2.900845
131.764239	2776.497850	5.977882	-0.026338	2.904762
131.670355	2784.614465	5.982886	-0.026326	2.908703
131.825281	2792.711419	5.987891	-0.026360	2.912642
132.108866	2800.763399	5.992896	-0.026418	2.916562
132.404369	2808.752803	5.997901	-0.026478	2.920446
132.762587	2816.705437	6.002906	-0.026550	2.924311
133.018554	2824.766659	6.007910	-0.026603	2.928217
132.999871	2832.835095	6.012915	-0.026605	2.932108
133.176337	2840.874165	6.017920	-0.026643	2.935989
133.540178	2848.871115	6.022925	-0.026716	2.939855
133.804228	2856.887027	6.027930	-0.026771	2.943719
134.140172	2864.931225	6.032934	-0.026839	2.947596
134.270099	2872.992191	6.037939	-0.026868	2.951465
134.636260	2881.029806	6.042944	-0.026942	2.955329
134.682837	2889.057031	6.047949	-0.026956	2.959167
134.813717	2897.088910	6.052954	-0.026985	2.963007
135.141767	2905.131733	6.057958	-0.027052	2.966857
135.057175	2913.187431	6.062963	-0.027041	2.970687
135.496084	2921.211251	6.067968	-0.027128	2.974524
135.661456	2929.242654	6.072973	-0.027164	2.978345
135.826525	2937.274615	6.077978	-0.027201	2.982162
135.829956	2945.361217	6.082982	-0.027207	2.985991
135.906618	2953.389656	6.087987	-0.027226	2.989792
136.491321	2961.435982	6.092992	-0.027340	2.993622
136.656440	2969.449931	6.097997	-0.027376	2.997410
136.803232	2977.486660	6.103002	-0.027409	3.001204
137.389179	2985.476695	6.108006	-0.027523	3.004992
137.605148	2993.502121	6.113011	-0.027569	3.008774
137.949484	3001.551566	6.118016	-0.027638	3.012569
137.951997	3009.641872	6.123021	-0.027644	3.016362
138.139238	3017.652960	6.128026	-0.027684	3.020121
138.387194	3025.689838	6.133030	-0.027736	3.023891
138.705594	3033.712809	6.138035	-0.027800	3.027653
139.123931	3041.760980	6.143040	-0.027884	3.031427
139.163574	3049.834617	6.148045	-0.027896	3.035189
139.236346	3057.840328	6.153050	-0.027915	3.038917
139.607365	3065.870754	6.158054	-0.027990	3.042667
139.789756	3073.905197	6.163059	-0.028029	3.046404
140.116902	3081.921872	6.168064	-0.028095	3.050135
140.162232	3089.998472	6.173069	-0.028109	3.053876
140.587134	3097.989926	6.178074	-0.028193	3.057592
140.984716	3106.050952	6.183078	-0.028273	3.061333
140.985786	3114.052240	6.188083	-0.028278	3.065024
141.234056	3122.119297	6.193088	-0.028330	3.068752
141.521202	3130.194373	6.198093	-0.028389	3.072481
141.687540	3138.245484	6.203098	-0.028425	3.076188
141.983869	3146.242153	6.208102	-0.028485	3.079872
142.213773	3154.230759	6.213107	-0.028534	3.083546
142.463006	3162.288460	6.218112	-0.028585	3.087247
142.740987	3170.295002	6.223117	-0.028642	3.090921
142.778920	3178.351832	6.228122	-0.028655	3.094603
142.983174	3186.385803	6.233126	-0.028698	3.098278
143.073568	3194.431946	6.238131	-0.028720	3.101949
143.576614	3202.402394	6.243136	-0.028819	3.105600
143.929296	3210.443561	6.248141	-0.028890	3.109272
143.973410	3218.519720	6.253146	-0.028904	3.112941
144.181632	3226.584266	6.258150	-0.028948	3.116608
144.370026	3234.557651	6.263155	-0.028988	3.120229
144.676265	3242.589455	6.268160	-0.029051	3.123877
144.882051	3250.646290	6.273165	-0.029094	3.127527
145.194929	3258.659852	6.278170	-0.029158	3.131159
145.718147	3266.698156	6.283174	-0.029260	3.134807
145.595979	3274.744442	6.288179	-0.029243	3.138425
146.140809	3282.742054	6.293184	-0.029350	3.142047
146.333155	3290.783744	6.298189	-0.029391	3.145669
146.547389	3298.814568	6.303194	-0.029436	3.149282
146.834928	3306.904710	6.308198	-0.029495	3.152922
146.960610	3314.921067	6.313203	-0.029524	3.156517
147.302917	3322.921366	6.318208	-0.029593	3.160110
147.573141	3330.921166	6.323213	-0.029648	3.163695
147.799575	3338.969430	6.328218	-0.029696	3.167297
148.082181	3347.027849	6.333222	-0.029754	3.170901
148.245619	3355.046745	6.338227	-0.029790	3.174478
148.691185	3363.058841	6.343232	-0.029878	3.178060
148.964214	3371.117888	6.348237	-0.029934	3.181652
149.062484	3379.136770	6.353242	-0.029958	3.185214
149.228466	3387.225865	6.358246	-0.029994	3.188806
149.483443	3395.225351	6.363251	-0.030047	3.192358
149.766705	3403.287697	6.368256	-0.030105	3.195935
150.083025	3411.276165	6.373261	-0.030169	3.199477
150.465623	3419.284347	6.378266	-0.030246	3.203027
150.972603	3427.321010	6.383270	-0.030345	3.206590
150.970001	3435.376030	6.388275	-0.030350	3.210136
151.720009	3443.386702	6.393280	-0.030495	3.213690
153.108026	3451.340856	6.398285	-0.030759	3.217241
153.535781	3459.370521	6.403290	-0.030844	3.220782
153.804470	3467.412040	6.408294	-0.030899	3.224317
153.812003	3475.475547	6.413299	-0.030906	3.227847
154.191697	3483.572428	6.418304	-0.030982	3.231404
154.352166	3491.657377	6.423309	-0.031017	3.234942
154.599860	3499.630757	6.428314	-0.031069	3.238431
154.923276	3507.653854	6.433318	-0.031134	3.241941
155.002339	3515.658935	6.438323	-0.031154	3.245429
155.806524	3523.643736	6.443328	-0.031309	3.248935
155.997879	3531.714203	6.448333	-0.031350	3.252448
156.014193	3539.780093	6.453338	-0.031358	3.255949
156.430326	3547.776896	6.458342	-0.031441	3.259433
156.718035	3555.792067	6.463347	-0.031500	3.262915
157.149526	3563.820855	6.468352	-0.031586	3.266405
157.067424	3571.880002	6.473357	-0.031576	3.269884
157.315173	3579.938658	6.478362	-0.031627	3.273372
157.796147	3587.968914	6.483366	-0.031722	3.276854
157.863425	3595.964952	6.488371	-0.031740	3.280300
158.028318	3603.991101	6.493376	-0.031776	3.283760
158.305844	3612.026537	6.498381	-0.031833	3.287225
158.399006	3620.063916	6.503386	-0.031856	3.290679
158.673093	3628.127764	6.508390	-0.031912	3.294148
158.902376	3636.125531	6.513395	-0.031960	3.297584
159.173750	3644.152074	6.518400	-0.032016	3.301030
159.221246	3652.167680	6.523405	-0.032030	3.304458
159.479410	3660.199932	6.528410	-0.032083	3.307899
160.125489	3668.240606	6.533414	-0.032209	3.311354
160.192315	3676.287142	6.538419	-0.032227	3.314786
160.404444	3684.313056	6.543424	-0.032272	3.318211
160.701829	3692.322218	6.548429	-0.032332	3.321629
160.951739	3700.324847	6.553434	-0.032384	3.325038
161.139982	3708.364053	6.558438	-0.032424	3.328458
161.412815	3716.400519	6.563443	-0.032481	3.331875
161.693330	3724.431429	6.568448	-0.032538	3.335287
161.760866	3732.481183	6.573453	-0.032556	3.338696
161.995037	3740.467044	6.578458	-0.032605	3.342080
162.336565	3748.510222	6.583462	-0.032674	3.345489
162.342066	3756.551679	6.588467	-0.032680	3.348881
162.399127	3764.626486	6.593472	-0.032696	3.352286
162.850318	3772.651758	6.598477	-0.032786	3.355681
163.207133	3780.619979	6.603482	-0.032857	3.359045
163.872672	3788.654583	6.608486	-0.032986	3.362445
164.361679	3796.635382	6.613491	-0.033083	3.365812
164.858764	3804.673638	6.618496	-0.033181	3.369200
165.050077	3812.763489	6.623501	-0.033222	3.372595
165.444881	3820.780056	6.628506	-0.033301	3.375963
165.835984	3828.779730	6.633510	-0.033379	3.379321
165.938532	3836.803792	6.638515	-0.033403	3.382675
166.276878	3844.831651	6.643520	-0.033471	3.386036
166.693777	3852.871517	6.648525	-0.033554	3.389401
166.965599	3860.953553	6.653530	-0.033610	3.392776
167.114107	3869.050376	6.658534	-0.033643	3.396148
167.531451	3876.981687	6.663539	-0.033726	3.399458
168.046602	3884.959408	6.668544	-0.033827	3.402787
168.346837	3893.000031	6.673549	-0.033889	3.406132
168.540285	3901.000289	6.678554	-0.033930	3.409453
168.917299	3909.065659	6.683558	-0.034006	3.412804
169.339655	3917.077212	6.688563	-0.034089	3.416131
169.488763	3925.092138	6.693568	-0.034123	3.419446
169.894860	3933.123255	6.698573	-0.034203	3.422774
169.910496	3941.150554	6.703578	-0.034212	3.426084
170.206636	3949.197501	6.708582	-0.034272	3.429408
170.353121	3957.239600	6.713587	-0.034305	3.432721
170.605326	3965.297630	6.718592	-0.034357	3.436042
171.005444	3973.277746	6.723597	-0.034437	3.439332
171.061126	3981.282271	6.728602	-0.034453	3.442618
171.208225	3989.351082	6.733606	-0.034485	3.445930
171.455024	3997.322021	6.738611	-0.034536	3.449201
171.693229	4005.420465	6.743616	-0.034586	3.452522
171.983354	4013.441625	6.748621	-0.034646	3.455809
172.220696	4021.449557	6.753626	-0.034695	3.459087
172.396931	4029.483881	6.758630	-0.034733	3.462369
172.495335	4037.505310	6.763635	-0.034757	3.465641
172.891618	4045.525972	6.768640	-0.034836	3.468919
173.110004	4053.613102	6.773645	-0.034882	3.472216
173.115961	4061.636474	6.778650	-0.034888	3.475476
173.488980	4069.634498	6.783654	-0.034963	3.478735
173.637736	4077.637879	6.788659	-0.034996	3.481985
173.861271	4085.627509	6.793664	-0.035043	3.485230
174.122033	4093.688129	6.798669	-0.035097	3.488501
174.368305	4101.701197	6.803674	-0.035148	3.491749
174.812043	4109.748934	6.808678	-0.035236	3.495015
175.069514	4117.746970	6.813683	-0.035289	3.498251
175.183717	4125.790789	6.818688	-0.035316	3.501499
175.481280	4133.775195	6.823693	-0.035377	3.504725
175.631427	4141.800236	6.828698	-0.035410	3.507960
176.020309	4149.888120	6.833702	-0.035488	3.511225
176.172544	4157.907871	6.838707	-0.035521	3.514452
176.296326	4165.935699	6.843712	-0.035550	3.517678
176.603642	4173.959240	6.848717	-0.035612	3.520905
176.797390	4181.933485	6.853722	-0.035653	3.524106
177.074689	4189.985175	6.858726	-0.035710	3.527338
177.181899	4197.994834	6.863731	-0.035736	3.530545
177.655095	4206.046618	6.868736	-0.035829	3.533776
177.912120	4214.082442	6.873741	-0.035882	3.536992
177.941033	4222.096705	6.878746	-0.035893	3.540189
178.231432	4230.118157	6.883750	-0.035952	3.543394
178.503396	4238.152318	6.888755	-0.036008	3.546601
178.790118	4246.176286	6.893760	-0.036067	3.549801
179.014818	4254.297152	6.898765	-0.036114	3.553034
179.254001	4262.333189	6.903770	-0.036164	3.556232
179.414119	4270.282443	6.908774	-0.036199	3.559390
179.566801	4278.290615	6.913779	-0.036233	3.562568
179.954596	4286.273660	6.918784	-0.036310	3.565740
180.242830	4294.307651	6.923789	-0.036369	3.568927
180.300938	4302.341373	6.928794	-0.036386	3.572104
180.724847	4310.361801	6.933798	-0.036470	3.575283
181.064033	4318.385470	6.938803	-0.036538	3.578459
181.206324	4326.424439	6.943808	-0.036570	3.581632
181.333274	4334.430484	6.948813	-0.036599	3.584788
181.765792	4342.438960	6.953818	-0.036685	3.587952
182.067306	4350.495960	6.958822	-0.036746	3.591128
182.324119	4358.506205	6.963827	-0.036799	3.594281
182.439190	4366.522660	6.968832	-0.036826	3.597431
183.051843	4374.528833	6.973837	-0.036946	3.600587
182.880139	4382.529052	6.978842	-0.036919	3.603716
183.114216	4390.594191	6.983846	-0.036968	3.606879
183.260930	4398.596861	6.988851	-0.037000	3.610013
183.716301	4406.629428	6.993856	-0.037091	3.613164
183.785310	4414.726158	6.998861	-0.037109	3.616327
184.007894	4422.665424	7.003866	-0.037155	3.619429
184.424893	4430.736591	7.008870	-0.037238	3.622586
184.638917	4438.715320	7.013875	-0.037284	3.625698
184.954747	4446.772570	7.018880	-0.037348	3.628841
185.383783	4454.829058	7.023885	-0.037433	3.631984
185.562619	4462.872330	7.028890	-0.037472	3.635112
185.903456	4470.858248	7.033894	-0.037540	3.638220
185.975340	4478.897155	7.038899	-0.037559	3.641338
186.138636	4486.859271	7.043904	-0.037595	3.644426
186.394981	4494.939655	7.048909	-0.037648	3.647560
186.857841	4502.909547	7.053914	-0.037739	3.650654
186.993710	4511.013076	7.058918	-0.037770	3.653788
186.917903	4519.047442	7.063923	-0.037761	3.656888
187.187404	4527.025428	7.068928	-0.037817	3.659972
187.688683	4535.078039	7.073933	-0.037915	3.663088
187.507968	4543.088941	7.078938	-0.037887	3.666167
187.749579	4551.097515	7.083942	-0.037937	3.669254
188.108996	4559.145658	7.088947	-0.038009	3.672357
188.279401	4567.176034	7.093952	-0.038047	3.675445
188.517180	4575.168045	7.098957	-0.038096	3.678518
188.622106	4583.174891	7.103962	-0.038121	3.681590
189.088208	4591.169369	7.108966	-0.038213	3.684664
189.214470	4599.240587	7.113971	-0.038242	3.687757
189.536401	4607.242828	7.118976	-0.038307	3.690825
189.848771	4615.300737	7.123981	-0.038371	3.693912
189.892831	4623.306250	7.128986	-0.038384	3.696969
190.410541	4631.289859	7.133990	-0.038486	3.700027
190.524803	4639.320580	7.138995	-0.038512	3.703091
190.771385	4647.360879	7.144000	-0.038564	3.706159
191.114189	4655.383655	7.149005	-0.038633	3.709220
191.146282	4663.432498	7.154010	-0.038644	3.712281
191.571012	4671.551480	7.159014	-0.038729	3.715376
191.642926	4679.484515	7.164019	-0.038747	3.718388
191.827057	4687.481889	7.169024	-0.038787	3.721426
192.143326	4695.462603	7.174029	-0.038851	3.724457
192.421495	4703.463943	7.179034	-0.038908	3.727494
192.569366	4711.525623	7.184038	-0.038941	3.730547
192.605907	4719.579548	7.189043	-0.038953	3.733592
192.867959	4727.627487	7.194048	-0.039007	3.736638
193.270745	4735.586356	7.199053	-0.039087	3.739651
193.237877	4743.617267	7.204058	-0.039087	3.742678
193.744227	4751.624258	7.209062	-0.039186	3.745707
193.745487	4759.676094	7.214067	-0.039192	3.748738
194.169689	4767.721449	7.219072	-0.039276	3.751774
194.364146	4775.770302	7.224077	-0.039318	3.754804
194.516494	4783.757655	7.229082	-0.039351	3.757807
194.687089	4791.790301	7.234086	-0.039388	3.760825
194.684174	4799.773491	7.239091	-0.039393	3.763818
194.940652	4807.834706	7.244096	-0.039446	3.766844
195.176068	4815.842899	7.249101	-0.039495	3.769847
195.168743	4823.899903	7.254106	-0.039499	3.772860
195.765821	4831.913352	7.259110	-0.039616	3.775869
195.995507	4839.912162	7.264115	-0.039664	3.778861
196.076056	4847.941467	7.269120	-0.039684	3.781859
196.624494	4855.914756	7.274125	-0.039792	3.784844
196.890308	4863.954251	7.279130	-0.039846	3.787844
197.041559	4872.038123	7.284134	-0.039880	3.790857
197.212322	4880.093750	7.289139	-0.039917	3.793857
197.630999	4888.074758	7.294144	-0.040000	3.796832
197.877625	4896.046300	7.299149	-0.040051	3.799798
198.125867	4904.057758	7.304154	-0.040103	3.802776
198.323468	4912.095431	7.309158	-0.040145	3.805760
198.495648	4920.124130	7.314163	-0.040183	3.808738
198.707767	4928.134088	7.319168	-0.040227	3.811708
198.891381	4936.204400	7.324173	-0.040267	3.814697
199.068106	4944.180966	7.329178	-0.040305	3.817649
199.441399	4952.224337	7.334182	-0.040380	3.820627
199.386320	4960.223452	7.339187	-0.040375	3.823578
199.743949	4968.239812	7.344192	-0.040447	3.826541
199.932096	4976.250186	7.349197	-0.040487	3.829496
200.022747	4984.282565	7.354202	-0.040509	3.832455
200.559701	4992.314569	7.359206	-0.040615	3.835421
200.767795	5000.280699	7.364211	-0.040659	3.838354
200.951618	5008.351323	7.369216	-0.040698	3.841322
201.357354	5016.346891	7.374221	-0.040779	3.844265
201.728089	5024.376277	7.379226	-0.040853	3.847217
201.916322	5032.406827	7.384230	-0.040894	3.850163
202.216764	5040.451886	7.389235	-0.040955	3.853115
202.456903	5048.495493	7.394240	-0.041005	3.856063
202.935083	5056.478419	7.399245	-0.041099	3.858991
202.826127	5064.537501	7.404250	-0.041084	3.861933
203.267585	5072.514371	7.409254	-0.041172	3.864854
203.526296	5080.562244	7.414259	-0.041225	3.867794
203.734821	5088.570244	7.419264	-0.041270	3.870717
204.066649	5096.802400	7.424269	-0.041337	3.873722
204.260737	5104.814234	7.429274	-0.041378	3.876641
204.528649	5112.714855	7.434278	-0.041433	3.879519
204.770458	5120.707955	7.439283	-0.041484	3.882428
205.079146	5128.683808	7.444288	-0.041546	3.885330
205.255923	5136.720124	7.449293	-0.041585	3.888249
205.346561	5144.741284	7.454298	-0.041607	3.891159
205.717696	5152.798514	7.459302	-0.041681	3.894085
205.973675	5160.818851	7.464307	-0.041734	3.896993
206.134527	5168.779480	7.469312	-0.041770	3.899876
206.423569	5176.795546	7.474317	-0.041829	3.902778
206.403648	5184.817353	7.479322	-0.041830	3.905675
206.950342	5192.839981	7.484326	-0.041937	3.908581
206.892600	5200.900027	7.489331	-0.041932	3.911487
207.115890	5208.922128	7.494336	-0.041979	3.914382
207.568434	5216.931585	7.499341	-0.042068	3.917274
207.565982	5224.906159	7.504346	-0.042073	3.920144
207.703483	5232.928976	7.509350	-0.042104	3.923031
208.122696	5240.951321	7.514355	-0.042188	3.925921
208.502946	5248.941716	7.519360	-0.042264	3.928797
208.523459	5257.031954	7.524365	-0.042273	3.931699
208.797918	5265.000475	7.529370	-0.042329	3.934561
209.225379	5273.035294	7.534374	-0.042414	3.937447
209.714599	5281.060042	7.539379	-0.042510	3.940328
209.731313	5289.082829	7.544384	-0.042519	3.943198
210.039972	5297.138153	7.549389	-0.042582	3.946083
210.318690	5305.110042	7.554394	-0.042639	3.948935
210.589754	5313.202826	7.559398	-0.042695	3.951829
210.934320	5321.193877	7.564403	-0.042764	3.954685
210.942691	5329.227321	7.569408	-0.042771	3.957548
211.198486	5337.229209	7.574413	-0.042824	3.960402
211.214018	5345.200277	7.579418	-0.042832	3.963239
211.535608	5353.251105	7.584422	-0.042897	3.966107
211.673829	5361.251621	7.589427	-0.042928	3.968953
211.739666	5369.281613	7.594432	-0.042946	3.971805
212.359832	5377.349263	7.599437	-0.043067	3.974678
212.512252	5385.334973	7.604442	-0.043100	3.977513
212.876666	5393.343822	7.609446	-0.043174	3.980356
213.167833	5401.314353	7.614451	-0.043233	3.983183
213.313259	5409.367195	7.619456	-0.043266	3.986035
213.324265	5417.403838	7.624461	-0.043273	3.988877
213.518202	5425.443967	7.629466	-0.043314	3.991721
213.846917	5433.510261	7.634470	-0.043381	3.994574
214.023249	5441.520396	7.639475	-0.043419	3.997403
214.165473	5449.477603	7.644480	-0.043451	4.000210
214.536797	5457.525811	7.649485	-0.043525	4.003052
214.755704	5465.490091	7.654490	-0.043571	4.005859
214.990562	5473.545453	7.659494	-0.043620	4.008696
215.340347	5481.602368	7.664499	-0.043691	4.011534
215.652589	5489.592141	7.669504	-0.043754	4.014346
215.633054	5497.671781	7.674509	-0.043756	4.017182
216.015282	5505.613836	7.679514	-0.043832	4.019974
216.466534	5513.662779	7.684518	-0.043922	4.022803
216.374642	5521.674521	7.689523	-0.043910	4.025608
216.679769	5529.683419	7.694528	-0.043972	4.028416
217.244298	5537.756414	7.699533	-0.044082	4.031249
217.184810	5545.873929	7.704538	-0.044077	4.034085
217.500903	5553.871004	7.709542	-0.044141	4.036883
217.803834	5561.781284	7.714547	-0.044203	4.039649
218.076525	5569.798682	7.719552	-0.044259	4.042450
218.197436	5577.789682	7.724557	-0.044286	4.045237
218.291584	5585.807106	7.729562	-0.044309	4.048031
218.701031	5593.846459	7.734566	-0.044391	4.050836
218.945240	5601.894891	7.739571	-0.044442	4.053639
218.925903	5609.903387	7.744576	-0.044443	4.056423
219.229653	5617.894090	7.749581	-0.044505	4.059203
219.497601	5625.918874	7.754586	-0.044560	4.061992
219.743546	5633.920489	7.759590	-0.044612	4.064772
219.928772	5641.941885	7.764595	-0.044651	4.067555
219.997700	5649.964578	7.769600	-0.044669	4.070335
220.562482	5658.025032	7.774605	-0.044780	4.073133
220.824874	5665.990614	7.779610	-0.044834	4.075893
221.005669	5673.983052	7.784614	-0.044873	4.078658
221.035525	5682.068386	7.789619	-0.044884	4.081452
221.133444	5690.019068	7.794624	-0.044907	4.084198
221.469783	5698.115092	7.799629	-0.044975	4.086995
221.587308	5706.100407	7.804634	-0.045003	4.089750
221.624281	5714.136014	7.809638	-0.045015	4.092519
221.864756	5722.158274	7.814643	-0.045065	4.095284
222.221588	5730.155229	7.819648	-0.045137	4.098040
222.473902	5738.163571	7.824653	-0.045189	4.100797
222.500859	5746.171516	7.829658	-0.045199	4.103549
222.916513	5754.226413	7.834662	-0.045282	4.106320
223.206911	5762.237076	7.839667	-0.045341	4.109072
223.480651	5770.283924	7.844672	-0.045398	4.111835
223.798636	5778.369279	7.849677	-0.045462	4.114609
223.840134	5786.369328	7.854682	-0.045475	4.117349
224.056018	5794.351816	7.859686	-0.045521	4.120083
224.459915	5802.322701	7.864691	-0.045601	4.122814
224.702521	5810.342452	7.869696	-0.045652	4.125558
224.922289	5818.360254	7.874701	-0.045698	4.128298
224.870485	5826.400693	7.879706	-0.045694	4.131042
225.232857	5834.461682	7.884710	-0.045766	4.133795
225.263956	5842.506232	7.889715	-0.045778	4.136537
225.355587	5850.449437	7.894720	-0.045800	4.139244
225.626210	5858.503451	7.899725	-0.045856	4.141988
225.930699	5866.447872	7.904730	-0.045918	4.144694
226.074179	5874.540192	7.909734	-0.045950	4.147447
226.255686	5882.553875	7.914739	-0.045989	4.150171
226.653177	5890.581018	7.919744	-0.046068	4.152900
226.935572	5898.677445	7.924749	-0.046126	4.155650
226.897542	5906.592335	7.929754	-0.046124	4.158333
227.180386	5914.612873	7.934758	-0.046182	4.161054
227.508238	5922.626182	7.939763	-0.046248	4.163770
227.665804	5930.631252	7.944768	-0.046283	4.166481
227.983751	5938.667609	7.949773	-0.046348	4.169201
228.116350	5946.702621	7.954778	-0.046378	4.171918
228.338845	5954.712193	7.959782	-0.046424	4.174625
228.673836	5962.766838	7.964787	-0.046492	4.177347
228.795361	5970.732035	7.969792	-0.046520	4.180034
228.877251	5978.793600	7.974797	-0.046541	4.182752
228.975351	5986.737519	7.979802	-0.046564	4.185428
229.381295	5994.782402	7.984806	-0.046645	4.188140
229.538412	6002.840668	7.989811	-0.046680	4.190853
229.582580	6010.916193	7.994816	-0.046693	4.193567
229.818028	6018.960228	7.999821	-0.046742	4.196272
230.138111	6026.872922	8.004826	-0.046807	4.198932
230.359923	6034.905559	8.009830	-0.046854	4.201629
230.200013	6042.874305	8.014835	-0.046829	4.204299
230.462253	6050.913288	8.019840	-0.046883	4.206995
231.130275	6058.901224	8.024845	-0.047013	4.209676
231.038281	6066.904697	8.029850	-0.047001	4.212353
231.130768	6074.977672	8.034854	-0.047024	4.215054
231.389269	6083.006939	8.039859	-0.047077	4.217740
231.462884	6090.977781	8.044864	-0.047096	4.220403
231.890965	6099.007701	8.049869	-0.047181	4.223087
231.863002	6107.003036	8.054874	-0.047181	4.225753
232.086990	6115.035362	8.059878	-0.047228	4.228433
232.260189	6123.049990	8.064883	-0.047266	4.231104
232.350924	6131.114369	8.069888	-0.047288	4.233790
232.842405	6139.159226	8.074893	-0.047385	4.236471
232.958793	6147.110221	8.079898	-0.047412	4.239116
233.150493	6155.138348	8.084902	-0.047453	4.241785
233.333693	6163.109785	8.089907	-0.047492	4.244434
233.410641	6171.124081	8.094912	-0.047512	4.247094
233.640667	6179.182498	8.099917	-0.047560	4.249769
234.142681	6187.219730	8.104922	-0.047659	4.252437
234.485430	6195.265651	8.109926	-0.047728	4.255105
234.528419	6203.266441	8.114931	-0.047741	4.257754
234.613850	6211.259761	8.119936	-0.047763	4.260399
234.921967	6219.327683	8.124941	-0.047825	4.263069
235.097103	6227.327775	8.129946	-0.047863	4.265713
235.051990	6235.357657	8.134950	-0.047860	4.268364
235.258485	6243.365089	8.139955	-0.047904	4.271008
235.659424	6251.402808	8.144960	-0.047984	4.273662
235.901940	6259.478224	8.149965	-0.048034	4.276326
236.090901	6267.405596	8.154970	-0.048075	4.278938
236.360760	6275.468667	8.159974	-0.048130	4.281594
236.437265	6283.422129	8.164979	-0.048150	4.284211
236.738453	6291.486000	8.169984	-0.048211	4.286865
236.936606	6299.496727	8.174989	-0.048254	4.289498
237.200241	6307.504188	8.179994	-0.048308	4.292129
237.617517	6315.522427	8.184998	-0.048391	4.294764
237.899057	6323.586210	8.190003	-0.048449	4.297410
237.831635	6331.545340	8.195008	-0.048441	4.300018
238.100715	6339.598487	8.200013	-0.048497	4.302658
238.182054	6347.578145	8.205018	-0.048517	4.305270
238.448384	6355.608934	8.210022	-0.048572	4.307899
238.646872	6363.606207	8.215027	-0.048614	4.310515
238.688542	6371.677055	8.220032	-0.048628	4.313152
239.069120	6379.701090	8.225037	-0.048704	4.315775
239.156738	6387.675584	8.230042	-0.048725	4.318378
239.216159	6395.682382	8.235046	-0.048742	4.320989
239.477445	6403.694330	8.240051	-0.048796	4.323603
239.827539	6411.692970	8.245056	-0.048866	4.326210
240.100038	6419.750097	8.250061	-0.048922	4.328835
240.421371	6427.762209	8.255066	-0.048987	4.331444
240.624846	6435.786636	8.260070	-0.049031	4.334054
240.907796	6443.821980	8.265075	-0.049089	4.336667
240.770723	6451.755788	8.270080	-0.049068	4.339242
241.225085	6459.874299	8.275085	-0.049158	4.341880
241.262968	6467.829433	8.280090	-0.049171	4.344460
241.371995	6475.839879	8.285094	-0.049196	4.347058
241.629872	6483.882978	8.290099	-0.049250	4.349665
241.830906	6491.938916	8.295104	-0.049292	4.352274
241.977308	6500.034655	8.300109	-0.049325	4.354894
241.929696	6508.000109	8.305114	-0.049321	4.357470
242.246419	6515.937015	8.310118	-0.049386	4.360037
242.381029	6523.966399	8.315123	-0.049416	4.362631
242.570356	6531.946356	8.320128	-0.049457	4.365208
242.833519	6540.006185	8.325133	-0.049511	4.367809
243.161206	6548.006751	8.330138	-0.049577	4.370390
243.321621	6556.013370	8.335142	-0.049612	4.372971
243.619699	6564.045524	8.340147	-0.049673	4.375559
243.743876	6572.031396	8.345152	-0.049702	4.378130
243.983115	6580.062661	8.350157	-0.049751	4.380714
244.254688	6588.039900	8.355162	-0.049807	4.383280
244.282243	6596.086519	8.360166	-0.049818	4.385865
244.660577	6604.145386	8.365171	-0.049894	4.388454
244.863356	6612.107090	8.370176	-0.049937	4.391010
244.886104	6620.202234	8.375181	-0.049946	4.393606
245.051514	6628.218888	8.380186	-0.049982	4.396176
245.164071	6636.186589	8.385190	-0.050008	4.398729
245.544817	6644.259906	8.390195	-0.050085	4.401315
245.699748	6652.194412	8.395200	-0.050119	4.403854
245.892924	6660.264814	8.400205	-0.050160	4.406435
246.079885	6668.247284	8.405210	-0.050200	4.408987
246.320810	6676.298153	8.410214	-0.050250	4.411559
246.445289	6684.325302	8.415219	-0.050279	4.414122
246.410017	6692.357668	8.420224	-0.050278	4.416684
246.828776	6700.356461	8.425229	-0.050361	4.419235
247.037971	6708.393574	8.430234	-0.050405	4.421797
247.151757	6716.354462	8.435238	-0.050432	4.424332
247.353792	6724.446259	8.440243	-0.050475	4.426908
247.527693	6732.432304	8.445248	-0.050512	4.429449
247.788278	6740.487609	8.450253	-0.050566	4.432011
247.741335	6748.531343	8.455258	-0.050563	4.434566
248.105071	6756.494367	8.460262	-0.050636	4.437095
248.373985	6764.483061	8.465267	-0.050691	4.439631
248.552309	6772.485529	8.470272	-0.050730	4.442170
248.694341	6780.467513	8.475277	-0.050761	4.444700
248.823474	6788.556812	8.480282	-0.050791	4.447263
249.023126	6796.513799	8.485286	-0.050833	4.449783
249.310871	6804.593703	8.490291	-0.050892	4.452341
249.561747	6812.548468	8.495296	-0.050944	4.454857
249.711429	6820.650386	8.500301	-0.050977	4.457418
249.823869	6828.576537	8.505306	-0.051004	4.459922
250.181532	6836.613114	8.510310	-0.051075	4.462460
250.576414	6844.622306	8.515315	-0.051154	4.464988
250.854226	6852.658343	8.520320	-0.051211	4.467523
250.975446	6860.695870	8.525325	-0.051239	4.470056
251.265607	6868.729202	8.530330	-0.051299	4.472587
251.415279	6876.743929	8.535334	-0.051332	4.475110
251.460544	6884.783223	8.540339	-0.051346	4.477639
251.526470	6892.712644	8.545344	-0.051363	4.480133
251.821568	6900.727641	8.550349	-0.051423	4.482652
252.068098	6908.756712	8.555354	-0.051475	4.485174
252.208386	6916.780514	8.560359	-0.051506	4.487693
252.402233	6924.801399	8.565363	-0.051547	4.490210
252.549475	6932.829303	8.570368	-0.051580	4.492727
252.731352	6940.894344	8.575373	-0.051619	4.495255
252.941201	6948.886962	8.580378	-0.051664	4.497758
253.116302	6956.859489	8.585383	-0.051702	4.500254
253.411210	6964.891381	8.590387	-0.051762	4.502767
253.648091	6972.870442	8.595392	-0.051811	4.505262
254.019751	6980.949854	8.600397	-0.051886	4.507788
253.811980	6988.932661	8.605402	-0.051852	4.510280
254.095878	6997.018967	8.610407	-0.051911	4.512804
254.353749	7005.071077	8.615411	-0.051964	4.515317
254.343999	7012.997574	8.620416	-0.051967	4.517788
254.684398	7020.988982	8.625421	-0.052036	4.520278
254.835043	7029.025409	8.630426	-0.052069	4.522781
255.129190	7036.990100	8.635431	-0.052129	4.525261
255.194346	7045.020067	8.640435	-0.052147	4.527759
255.283409	7052.955902	8.645440	-0.052169	4.530226
255.627332	7061.078406	8.650445	-0.052238	4.532751
255.794886	7069.089015	8.655450	-0.052275	4.535238
255.926984	7077.102296	8.660455	-0.052305	4.537726
256.239952	7085.139120	8.665459	-0.052368	4.540219
256.270237	7093.131711	8.670464	-0.052379	4.542697
256.469720	7101.136842	8.675469	-0.052421	4.545178
256.790523	7109.157901	8.680474	-0.052487	4.547662
257.048102	7117.151510	8.685479	-0.052540	4.550137
257.122785	7125.236271	8.690483	-0.052559	4.552638
257.316349	7133.210826	8.695488	-0.052600	4.555104
257.570875	7141.305739	8.700493	-0.052653	4.557605
257.583313	7149.225229	8.705498	-0.052661	4.560051
257.583947	7157.246157	8.710503	-0.052666	4.562527
258.170887	7165.240851	8.715507	-0.052781	4.564994
258.183328	7173.324246	8.720512	-0.052788	4.567486
258.250836	7181.303443	8.725517	-0.052806	4.569945
258.581442	7189.390553	8.730522	-0.052873	4.572436
258.842361	7197.372856	8.735527	-0.052927	4.574894
258.904617	7205.445397	8.740531	-0.052944	4.577377
258.956124	7213.325352	8.745536	-0.052959	4.579800
259.359171	7221.449467	8.750541	-0.053039	4.582297
259.497911	7229.398823	8.755546	-0.053070	4.584739
259.714941	7237.458111	8.760551	-0.053116	4.587213
260.085897	7245.476767	8.765555	-0.053190	4.589673
260.345665	7253.540804	8.770560	-0.053244	4.592146
260.797601	7261.581497	8.775565	-0.053334	4.594611
260.951972	7269.563872	8.780570	-0.053368	4.597056
261.180356	7277.485200	8.785575	-0.053415	4.599481
261.545520	7285.549480	8.790579	-0.053489	4.601949
261.431683	7293.468476	8.795584	-0.053473	4.604371
261.803947	7301.592620	8.800589	-0.053547	4.606854
261.800144	7309.564001	8.805594	-0.053552	4.609289
262.023130	7317.620373	8.810599	-0.053599	4.611749
262.478137	7325.659665	8.815603	-0.053689	4.614202
262.438479	7333.665411	8.820608	-0.053687	4.616644
262.652522	7341.649891	8.825613	-0.053732	4.619078
262.803616	7349.632482	8.830618	-0.053765	4.621510
263.163492	7357.643107	8.835623	-0.053838	4.623949
263.368689	7365.729776	8.840627	-0.053881	4.626410
263.495582	7373.688308	8.845632	-0.053910	4.628831
263.597199	7381.765042	8.850637	-0.053934	4.631286
263.801710	7389.785643	8.855642	-0.053978	4.633723
263.798204	7397.784468	8.860647	-0.053982	4.636153
264.134900	7405.793323	8.865651	-0.054050	4.638583
264.183876	7413.767798	8.870656	-0.054065	4.641003
264.250847	7421.750623	8.875661	-0.054083	4.643423
264.734045	7429.819100	8.880666	-0.054178	4.645868
264.963237	7437.824301	8.885671	-0.054226	4.648292
265.339293	7445.852785	8.890675	-0.054301	4.650723
265.485783	7453.855994	8.895680	-0.054334	4.653144
265.844879	7461.902361	8.900685	-0.054406	4.655577
266.120756	7469.907328	8.905690	-0.054463	4.657996
266.141832	7477.881499	8.910695	-0.054472	4.660405
266.485493	7485.936591	8.915699	-0.054541	4.662837
266.422224	7493.899135	8.920704	-0.054535	4.665240
266.471013	7501.971861	8.925709	-0.054549	4.667675
266.961513	7509.975217	8.930714	-0.054646	4.670087
267.126482	7518.050806	8.935719	-0.054682	4.672520
267.225102	7526.123090	8.940723	-0.054706	4.674951
267.334817	7534.079327	8.945728	-0.054731	4.677345
267.648476	7542.015865	8.950733	-0.054795	4.679732
267.664735	7550.033873	8.955738	-0.054803	4.682143
267.776301	7557.977600	8.960743	-0.054829	4.684530
267.939912	7566.074408	8.965747	-0.054865	4.686962
268.057937	7574.044149	8.970752	-0.054892	4.689354
268.364812	7582.114951	8.975757	-0.054955	4.691775
268.531908	7590.106879	8.980762	-0.054991	4.694172
268.712745	7598.132227	8.985767	-0.055030	4.696577
269.025072	7606.157460	8.990771	-0.055094	4.698981
269.249494	7614.140420	8.995776	-0.055141	4.701371
269.351624	7622.182993	9.000781	-0.055165	4.703777
269.497660	7630.211269	9.005786	-0.055198	4.706178
269.696585	7638.203379	9.010791	-0.055240	4.708567
269.872301	7646.209900	9.015795	-0.055278	4.710959
270.039957	7654.281146	9.020800	-0.055315	4.713370
270.199540	7662.293762	9.025805	-0.055350	4.715761
270.228565	7670.302085	9.030810	-0.055360	4.718150
270.301031	7678.279257	9.035815	-0.055379	4.720529
270.515523	7686.315178	9.040819	-0.055424	4.722924
270.687806	7694.291990	9.045824	-0.055462	4.725299
271.047725	7702.357478	9.050829	-0.055534	4.727700
271.344106	7710.380442	9.055834	-0.055595	4.730087
271.343087	7718.432017	9.060839	-0.055600	4.732482
271.623640	7726.441073	9.065843	-0.055657	4.734862
271.807649	7734.413372	9.070848	-0.055697	4.737230
272.136085	7742.439581	9.075853	-0.055763	4.739613
272.246338	7750.466642	9.080858	-0.055789	4.741995
272.509395	7758.399417	9.085863	-0.055843	4.744348
272.749371	7766.497111	9.090867	-0.055893	4.746749
272.726537	7774.471791	9.095872	-0.055894	4.749112
273.095587	7782.563400	9.100877	-0.055968	4.751508
273.265616	7790.592645	9.105882	-0.056005	4.753885
273.249783	7798.573181	9.110887	-0.056008	4.756247
273.650875	7806.566812	9.115891	-0.056088	4.758610
274.002712	7814.516457	9.120896	-0.056159	4.760959
273.962187	7822.560515	9.125901	-0.056156	4.763336
273.924795	7830.525093	9.130906	-0.056155	4.765688
274.121824	7838.580110	9.135911	-0.056197	4.768065
274.546066	7846.666470	9.140915	-0.056281	4.770450
274.476634	7854.645826	9.145920	-0.056273	4.772803
274.815689	7862.654594	9.150925	-0.056342	4.775162
275.130971	7870.643825	9.155930	-0.056406	4.777515
275.133983	7878.689108	9.160935	-0.056412	4.779884
275.331695	7886.676338	9.165939	-0.056454	4.782234
275.303701	7894.665502	9.170944	-0.056454	4.784584
275.720259	7902.739208	9.175949	-0.056537	4.786956
275.665344	7910.755089	9.180954	-0.056532	4.789312
275.728623	7918.722396	9.185959	-0.056549	4.791652
275.999251	7926.812616	9.190963	-0.056605	4.794026
275.831969	7934.791891	9.195968	-0.056579	4.796368
276.236010	7942.811307	9.200973	-0.056659	4.798718
276.411166	7950.843040	9.205978	-0.056697	4.801072
276.383487	7958.794651	9.210983	-0.056697	4.803402
276.346267	7966.837410	9.215987	-0.056696	4.805757
276.657743	7974.836294	9.220992	-0.056759	4.808097
276.979838	7982.862855	9.225997	-0.056824	4.810444
277.174554	7990.268825	9.231002	-0.056865	4.812609
277.366197	7994.794954	9.236007	-0.056904	4.813931

277.655144	7997.284416	9.241011	-0.056960	4.814657
277.736827	7998.496221	9.246016	-0.056976	4.815011
277.830514	7999.003132	9.251021	-0.056994	4.815158
278.060669	8000.011295	9.256026	-0.057037	4.815452
278.021267	8000.017064	9.261031	-0.057030	4.815454
278.035018	8000.016230	9.266035	-0.057033	4.815454
278.018239	7999.995659	9.271040	-0.057030	4.815448
278.194505	8000.045585	9.276045	-0.057063	4.815461
278.303975	8000.017477	9.281050	-0.057083	4.815453
278.232890	8000.018450	9.286055	-0.057070	4.815453
278.215003	8000.059835	9.291059	-0.057067	4.815465
278.196409	8000.041372	9.296064	-0.057063	4.815460
278.370058	8000.060268	9.301069	-0.057096	4.815465
278.382017	8000.062609	9.306074	-0.057098	4.815465
278.522239	8000.043557	9.311079	-0.057124	4.815459
278.587265	8000.063869	9.316083	-0.057136	4.815465
278.624324	8000.013198	9.321088	-0.057143	4.815450
278.719256	8000.082087	9.326093	-0.057161	4.815469
278.744631	8000.038703	9.331098	-0.057166	4.815457
278.743495	8000.024800	9.336103	-0.057166	4.815453
278.849564	8000.085325	9.341107	-0.057186	4.815470
278.711913	8000.047802	9.346112	-0.057160	4.815459
278.634623	8000.025166	9.351117	-0.057146	4.815453
278.830109	8000.010229	9.356122	-0.057182	4.815448
279.154835	8000.024136	9.361127	-0.057243	4.815450
279.017116	8000.035765	9.366131	-0.057217	4.815454
278.839339	8000.002924	9.371136	-0.057184	4.815446
278.959640	8000.039107	9.376141	-0.057207	4.815456
279.018439	8000.042220	9.381146	-0.057218	4.815456
279.033328	8000.030719	9.386151	-0.057221	4.815453
278.879974	8000.070941	9.391155	-0.057192	4.815465
278.968195	8000.036072	9.396160	-0.057209	4.815455
279.190586	8000.044019	9.401165	-0.057250	4.815456
279.243426	8000.035280	9.406170	-0.057260	4.815453
279.282802	8000.026320	9.411175	-0.057267	4.815450
279.137550	8000.012179	9.416179	-0.057240	4.815447
279.106329	8000.008467	9.421184	-0.057235	4.815446
279.465747	8000.028289	9.426189	-0.057302	4.815450
279.552284	8000.032928	9.431194	-0.057318	4.815451
279.360971	8000.020165	9.436199	-0.057282	4.815448
279.399676	8000.060347	9.441203	-0.057290	4.815460
279.329680	8000.027144	9.446208	-0.057277	4.815450
279.301389	8000.039508	9.451213	-0.057272	4.815454
279.179497	8000.035369	9.456218	-0.057249	4.815454
279.284582	8000.025355	9.461223	-0.057269	4.815450
279.570167	8000.032207	9.466227	-0.057322	4.815451
279.521454	8000.026068	9.471232	-0.057313	4.815449
279.396658	8000.065692	9.476237	-0.057290	4.815461
279.383321	8000.041972	9.481242	-0.057287	4.815454
279.416028	8000.037175	9.486247	-0.057294	4.815453
279.543896	8000.059593	9.491251	-0.057317	4.815459
279.425496	8000.015975	9.496256	-0.057295	4.815447
279.543717	8000.040371	9.501261	-0.057318	4.815453
279.513753	8000.021719	9.506266	-0.057312	4.815448
279.634436	8000.046156	9.511271	-0.057335	4.815454
279.622664	8000.047037	9.516275	-0.057332	4.815455
279.332484	8000.040125	9.521280	-0.057279	4.815454
279.616530	8000.074734	9.526285	-0.057332	4.815463
279.558936	8000.053489	9.531290	-0.057321	4.815457
279.407030	8000.031759	9.536295	-0.057293	4.815451
279.633197	8000.061139	9.541299	-0.057335	4.815459
279.620811	8000.027818	9.546304	-0.057333	4.815449
279.559336	8000.044977	9.551309	-0.057321	4.815454
279.386263	8000.045337	9.556314	-0.057289	4.815455
279.435253	8000.029055	9.561319	-0.057298	4.815450
279.795416	8000.068125	9.566323	-0.057366	4.815460
279.717782	8000.031590	9.571328	-0.057351	4.815450
280.021622	8000.054772	9.576333	-0.057408	4.815455
279.820791	8000.066429	9.581338	-0.057370	4.815459
279.934820	8000.053356	9.586343	-0.057392	4.815455
279.960566	8000.091188	9.591347	-0.057397	4.815466
279.876719	8000.085539	9.596352	-0.057381	4.815465
279.776402	8000.084961	9.601357	-0.057363	4.815465
280.051590	8000.083094	9.606362	-0.057414	4.815463
280.010048	8000.086691	9.611367	-0.057406	4.815464
280.110189	8000.081938	9.616371	-0.057425	4.815463
279.904744	8000.042227	9.621376	-0.057387	4.815452
279.959837	8000.085885	9.626381	-0.057397	4.815464
280.055177	8000.083190	9.631386	-0.057415	4.815463
279.842685	8000.065803	9.636391	-0.057375	4.815459
279.936950	8000.085530	9.641395	-0.057393	4.815464
280.002811	8000.032127	9.646400	-0.057405	4.815449
280.152808	8000.101927	9.651405	-0.057434	4.815468
280.227085	8000.098885	9.656410	-0.057447	4.815467
280.201051	8000.065337	9.661415	-0.057443	4.815457
280.290777	8000.102087	9.666419	-0.057459	4.815468
280.049955	8000.035078	9.671424	-0.057415	4.815449
280.163266	8000.077559	9.676429	-0.057436	4.815461
280.083734	8000.044199	9.681434	-0.057421	4.815452
279.973975	8000.076590	9.686439	-0.057401	4.815462
279.912934	8000.067043	9.691443	-0.057389	4.815459
279.933078	8000.066314	9.696448	-0.057393	4.815459
279.907953	8000.102238	9.701453	-0.057389	4.815469
279.914624	8000.051065	9.706458	-0.057390	4.815454
279.926298	8000.037373	9.711463	-0.057392	4.815450
280.043710	8000.083128	9.716467	-0.057414	4.815463
279.938895	8000.065378	9.721472	-0.057395	4.815459
280.116399	8000.105712	9.726477	-0.057428	4.815469
280.240513	8000.077846	9.731482	-0.057451	4.815461
280.185977	8000.066269	9.736487	-0.057441	4.815458
280.219814	8000.090343	9.741491	-0.057447	4.815464
280.255380	8000.039645	9.746496	-0.057454	4.815449
280.362837	8000.062796	9.751501	-0.057474	4.815456
280.131263	8000.070739	9.756506	-0.057431	4.815459
279.997698	8000.033282	9.761511	-0.057406	4.815449
280.259975	8000.060054	9.766515	-0.057455	4.815455
280.201958	8000.024910	9.771520	-0.057445	4.815445
280.200205	8000.052672	9.776525	-0.057444	4.815454
280.295387	8000.057454	9.781530	-0.057462	4.815454
280.066219	8000.059026	9.786535	-0.057420	4.815456
280.177782	8000.084381	9.791539	-0.057441	4.815463
280.194591	8000.063294	9.796544	-0.057444	4.815457
280.040024	8000.098153	9.801549	-0.057415	4.815468
280.060590	8000.073923	9.806554	-0.057419	4.815460
280.122727	8000.066406	9.811559	-0.057431	4.815458
280.278529	8000.094628	9.816563	-0.057460	4.815465
280.108244	8000.054428	9.821568	-0.057428	4.815454
280.076869	8000.064604	9.826573	-0.057422	4.815458
280.417078	8000.063810	9.831578	-0.057486	4.815456
280.267133	8000.043179	9.836583	-0.057458	4.815450
280.309184	8000.055634	9.841587	-0.057466	4.815454
280.449769	8000.022697	9.846592	-0.057492	4.815444
280.398732	8000.081703	9.851597	-0.057483	4.815461
280.224682	8000.039303	9.856602	-0.057450	4.815449
280.076904	8000.028325	9.861607	-0.057423	4.815447
280.156817	8000.084147	9.866611	-0.057438	4.815463
280.290816	8000.054307	9.871616	-0.057463	4.815454
280.240797	8000.091958	9.876621	-0.057454	4.815465
280.307204	8000.077032	9.881626	-0.057466	4.815460
280.441270	8000.072839	9.886631	-0.057491	4.815458
280.593030	8000.103132	9.891635	-0.057520	4.815466
280.590984	8000.072117	9.896640	-0.057519	4.815457
280.476173	8000.080917	9.901645	-0.057498	4.815460
280.314439	8000.060091	9.906650	-0.057468	4.815455
280.501531	8000.093104	9.911655	-0.057503	4.815464
280.689510	8000.112241	9.916659	-0.057538	4.815468
280.324395	8000.047455	9.921664	-0.057470	4.815451
280.299016	8000.051318	9.926669	-0.057465	4.815453
280.417626	8000.069310	9.931674	-0.057488	4.815457
280.283017	8000.053207	9.936679	-0.057463	4.815453
280.176944	8000.072836	9.941683	-0.057443	4.815459
280.178619	8000.079283	9.946688	-0.057443	4.815461
280.286787	8000.071457	9.951693	-0.057463	4.815459
280.389140	8000.056055	9.956698	-0.057483	4.815454
280.191281	8000.042114	9.961703	-0.057446	4.815450
280.521018	8000.053970	9.966707	-0.057507	4.815452
280.527124	8000.051941	9.971712	-0.057509	4.815452
280.389057	8000.088140	9.976717	-0.057483	4.815463
280.431187	8000.055717	9.981722	-0.057491	4.815453
280.557327	8000.040707	9.986727	-0.057514	4.815448
280.509216	8000.071978	9.991731	-0.057506	4.815458
280.375128	8000.027032	9.996736	-0.057481	4.815445
280.627536	8000.058985	10.001741	-0.057528	4.815453
280.582902	8000.055050	10.006746	-0.057520	4.815452
280.478345	8000.045853	10.011751	-0.057500	4.815450
280.668786	8000.102430	10.016755	-0.057536	4.815466
280.623890	8000.053611	10.021760	-0.057527	4.815452
280.557075	8000.069614	10.026765	-0.057515	4.815457
280.665846	8000.076758	10.031770	-0.057535	4.815458
280.572086	8000.059191	10.036775	-0.057518	4.815454
280.521483	8000.061569	10.041779	-0.057509	4.815454
280.557419	8000.032249	10.046784	-0.057515	4.815446
280.478318	8000.055530	10.051789	-0.057501	4.815453
280.746414	8000.051410	10.056794	-0.057551	4.815450
280.459426	8000.038136	10.061799	-0.057497	4.815448
280.632682	8000.079469	10.066803	-0.057530	4.815459
280.673491	8000.035269	10.071808	-0.057537	4.815446
280.625100	8000.071879	10.076813	-0.057529	4.815457
280.647878	8000.036999	10.081818	-0.057533	4.815447
280.641458	8000.065752	10.086823	-0.057532	4.815455
280.634768	8000.089158	10.091827	-0.057531	4.815462
280.612656	8000.050332	10.096832	-0.057527	4.815451
280.561982	8000.050572	10.101837	-0.057517	4.815451
280.682291	8000.084621	10.106842	-0.057540	4.815460
280.645089	8000.067986	10.111847	-0.057533	4.815456
280.641842	8000.073283	10.116851	-0.057532	4.815457
280.769890	8000.036933	10.121856	-0.057556	4.815446
280.775244	8000.062675	10.126861	-0.057557	4.815454
280.868151	8000.081312	10.131866	-0.057575	4.815459
280.964448	8000.066879	10.136871	-0.057593	4.815454
280.998435	8000.085613	10.141875	-0.057599	4.815459
280.828378	8000.077473	10.146880	-0.057568	4.815458
280.813145	8000.086846	10.151885	-0.057565	4.815460
280.742340	8000.075000	10.156890	-0.057552	4.815457
280.694226	8000.077420	10.161895	-0.057543	4.815458
280.863792	8000.095184	10.166899	-0.057575	4.815463
280.826549	8000.052903	10.171904	-0.057568	4.815450
280.824317	8000.067833	10.176909	-0.057567	4.815455
280.898246	8000.074403	10.181914	-0.057581	4.815456
280.883870	8000.056007	10.186919	-0.057579	4.815451
280.867049	8000.092069	10.191923	-0.057576	4.815462
280.684897	8000.044192	10.196928	-0.057542	4.815449
280.763456	8000.067935	10.201933	-0.057556	4.815455
280.906530	8000.094880	10.206938	-0.057583	4.815462
280.935033	8000.070780	10.211943	-0.057589	4.815455
280.986935	8000.075918	10.216947	-0.057598	4.815456
280.912620	8000.041573	10.221952	-0.057585	4.815447
280.810259	8000.055921	10.226957	-0.057566	4.815451
280.981076	8000.083324	10.231962	-0.057597	4.815459
280.983547	8000.064137	10.236967	-0.057598	4.815453
280.913132	8000.098247	10.241971	-0.057585	4.815463
280.932639	8000.069724	10.246976	-0.057589	4.815455
281.020932	8000.081874	10.251981	-0.057605	4.815458
281.121402	8000.065373	10.256986	-0.057624	4.815453
281.082801	8000.074361	10.261991	-0.057617	4.815455
280.861589	8000.093159	10.266995	-0.057576	4.815462
280.835825	8000.057479	10.272000	-0.057571	4.815452
280.865650	8000.052635	10.277005	-0.057577	4.815450
281.032181	8000.106682	10.282010	-0.057608	4.815465
280.981181	8000.080202	10.287015	-0.057598	4.815458
281.006111	8000.096649	10.292019	-0.057603	4.815462
280.848996	8000.088722	10.297024	-0.057574	4.815461
280.850696	8000.095169	10.302029	-0.057574	4.815463
280.928941	8000.141348	10.307034	-0.057589	4.815476
280.862373	8000.079348	10.312039	-0.057577	4.815458
281.080006	8000.128895	10.317043	-0.057617	4.815471
281.050802	8000.132695	10.322048	-0.057612	4.815473
281.117277	8000.120976	10.327053	-0.057624	4.815469
281.239438	8000.097352	10.332058	-0.057647	4.815461
281.118193	8000.072919	10.337063	-0.057625	4.815455
281.173897	8000.106972	10.342067	-0.057635	4.815464
280.935657	8000.065648	10.347072	-0.057591	4.815454
281.236301	8000.073821	10.352077	-0.057647	4.815454
281.279270	8000.108732	10.357082	-0.057655	4.815464
281.173668	8000.068528	10.362087	-0.057636	4.815453
281.060552	8000.116894	10.367091	-0.057615	4.815468
280.943585	8000.067953	10.372096	-0.057593	4.815454
281.235307	8000.102694	10.377101	-0.057647	4.815463
281.344831	8000.126949	10.382106	-0.057668	4.815469
281.186734	8000.077330	10.387111	-0.057638	4.815456
281.448884	8000.110514	10.392115	-0.057687	4.815464
281.419931	8000.080123	10.397120	-0.057682	4.815455
281.341237	8000.099136	10.402125	-0.057667	4.815461
281.247279	8000.078358	10.407130	-0.057650	4.815456
281.198637	8000.074357	10.412135	-0.057641	4.815455
281.327912	8000.113898	10.417139	-0.057665	4.815466
281.035352	8000.083433	10.422144	-0.057611	4.815458
281.177340	8000.121047	10.427149	-0.057637	4.815468
281.153559	8000.095015	10.432154	-0.057633	4.815461
281.164002	8000.096264	10.437159	-0.057635	4.815461
281.207124	8000.109806	10.442163	-0.057643	4.815465
281.156083	8000.072639	10.447168	-0.057634	4.815454
281.153716	8000.103597	10.452173	-0.057633	4.815464
281.401764	8000.108765	10.457178	-0.057680	4.815464
281.387080	8000.095707	10.462183	-0.057677	4.815460
281.257726	8000.090374	10.467187	-0.057653	4.815459
281.138341	8000.088412	10.472192	-0.057631	4.815459
281.155061	8000.107930	10.477197	-0.057634	4.815465
281.310050	8000.128661	10.482202	-0.057663	4.815470
281.121809	8000.083888	10.487207	-0.057628	4.815458
281.179335	8000.091256	10.492211	-0.057639	4.815460
281.230447	8000.075009	10.497216	-0.057648	4.815455
281.254550	8000.103197	10.502221	-0.057653	4.815463
281.082873	8000.116401	10.507226	-0.057621	4.815468
281.053332	8000.066766	10.512231	-0.057616	4.815453
281.186017	8000.127735	10.517235	-0.057640	4.815470
281.107653	8000.097598	10.522240	-0.057626	4.815462
281.051930	8000.118058	10.527245	-0.057616	4.815468
281.038164	8000.127456	10.532250	-0.057613	4.815471
280.966030	8000.083530	10.537255	-0.057600	4.815459
281.113910	8000.122309	10.542259	-0.057627	4.815469
281.117220	8000.095656	10.547264	-0.057628	4.815461
281.037572	8000.095418	10.552269	-0.057613	4.815462
281.165077	8000.109283	10.557274	-0.057637	4.815465
281.252127	8000.064777	10.562279	-0.057653	4.815452
281.332149	8000.104574	10.567283	-0.057668	4.815463
281.224695	8000.062202	10.572288	-0.057649	4.815451
281.397308	8000.077880	10.577293	-0.057681	4.815455
281.520386	8000.106634	10.582298	-0.057704	4.815463
281.208533	8000.064095	10.587303	-0.057646	4.815452
281.250282	8000.080820	10.592307	-0.057654	4.815456
281.159047	8000.060088	10.597312	-0.057637	4.815451
281.209471	8000.083368	10.602317	-0.057646	4.815457
281.304316	8000.102037	10.607322	-0.057664	4.815462
281.047477	8000.097808	10.612327	-0.057616	4.815462
281.217855	8000.130547	10.617331	-0.057648	4.815471
281.065818	8000.108811	10.622336	-0.057620	4.815465
281.237914	8000.107383	10.627341	-0.057652	4.815464
281.240940	8000.117058	10.632346	-0.057653	4.815467
281.044518	8000.066807	10.637351	-0.057616	4.815453
281.262833	8000.108885	10.642355	-0.057657	4.815464
281.421146	8000.108299	10.647360	-0.057686	4.815464
281.227672	8000.046341	10.652365	-0.057650	4.815446
281.269956	8000.089790	10.657370	-0.057658	4.815459
281.324369	8000.081078	10.662375	-0.057669	4.815456
281.136434	8000.105769	10.667379	-0.057634	4.815464
281.105812	8000.065733	10.672384	-0.057628	4.815453
281.284869	8000.081517	10.677389	-0.057662	4.815456
281.323964	8000.107816	10.682394	-0.057669	4.815464
281.304823	8000.065832	10.687399	-0.057665	4.815452
281.216010	8000.109256	10.692403	-0.057649	4.815465
281.353388	8000.071991	10.697408	-0.057675	4.815453
281.351803	8000.096551	10.702413	-0.057674	4.815460
281.337255	8000.119827	10.707418	-0.057672	4.815467
281.285353	8000.074097	10.712423	-0.057662	4.815454
281.409067	8000.108204	10.717427	-0.057685	4.815464
281.345332	8000.060141	10.722432	-0.057674	4.815450
281.382694	8000.080000	10.727437	-0.057681	4.815455
281.379298	8000.098117	10.732442	-0.057680	4.815461
281.242747	8000.075569	10.737447	-0.057655	4.815455
281.258725	8000.112172	10.742451	-0.057658	4.815465
281.301910	8000.070148	10.747456	-0.057666	4.815453
281.339954	8000.082538	10.752461	-0.057673	4.815456
281.411593	8000.092276	10.757466	-0.057686	4.815459
281.513013	8000.073653	10.762471	-0.057705	4.815453
281.451599	8000.088676	10.767475	-0.057694	4.815458
281.211660	8000.076177	10.772480	-0.057649	4.815455
281.306663	8000.087369	10.777485	-0.057667	4.815458
281.380554	8000.082184	10.782490	-0.057681	4.815456
281.215879	8000.078406	10.787495	-0.057651	4.815456
281.423233	8000.123510	10.792499	-0.057689	4.815468
281.365119	8000.116147	10.797504	-0.057678	4.815466
281.609275	8000.118045	10.802509	-0.057724	4.815465
281.589614	8000.119865	10.807514	-0.057720	4.815466
281.351835	8000.096715	10.812519	-0.057676	4.815460
281.425741	8000.147097	10.817523	-0.057690	4.815475
281.406762	8000.156409	10.822528	-0.057687	4.815478
281.361357	8000.125747	10.827533	-0.057678	4.815469
281.480225	8000.144813	10.832538	-0.057701	4.815474
281.407235	8000.113695	10.837543	-0.057687	4.815465
281.370670	8000.139814	10.842547	-0.057680	4.815473
281.382849	8000.153915	10.847552	-0.057683	4.815477
281.268816	8000.127463	10.852557	-0.057661	4.815470
281.293608	8000.146045	10.857562	-0.057666	4.815475
281.305244	8000.098158	10.862567	-0.057668	4.815461
281.600271	8000.124405	10.867571	-0.057723	4.815467
281.490882	8000.118333	10.872576	-0.057703	4.815466
281.521340	8000.104951	10.877581	-0.057709	4.815462
281.609995	8000.125656	10.882586	-0.057726	4.815468
281.385909	8000.097389	10.887591	-0.057684	4.815460
281.407984	8000.143710	10.892595	-0.057688	4.815474
281.391231	8000.130618	10.897600	-0.057685	4.815470
281.423620	8000.119405	10.902605	-0.057691	4.815467
281.421047	8000.119370	10.907610	-0.057691	4.815467
281.292714	8000.069173	10.912615	-0.057667	4.815453
281.353795	8000.116138	10.917619	-0.057678	4.815466
281.381274	8000.100570	10.922624	-0.057684	4.815461
281.305788	8000.108950	10.927629	-0.057670	4.815464
281.342008	8000.103143	10.932634	-0.057676	4.815462
281.431611	8000.062953	10.937639	-0.057693	4.815450
281.438723	8000.102616	10.942643	-0.057695	4.815462
281.402914	8000.107376	10.947648	-0.057688	4.815463
281.371618	8000.095112	10.952653	-0.057682	4.815460
281.400215	8000.096660	10.957658	-0.057688	4.815460
281.511729	8000.105988	10.962663	-0.057709	4.815462
281.607630	8000.107578	10.967667	-0.057726	4.815462
281.627167	8000.100427	10.972672	-0.057730	4.815460
281.591512	8000.136179	10.977677	-0.057724	4.815471
281.651212	8000.188465	10.982682	-0.057735	4.815486
281.541909	8000.112935	10.987687	-0.057715	4.815464
281.563516	8000.120779	10.992691	-0.057719	4.815466
281.615926	8000.107759	10.997696	-0.057729	4.815462
281.709485	8000.097556	11.002701	-0.057746	4.815459
281.658620	8000.122370	11.007706	-0.057737	4.815466
281.597575	8000.091450	11.012711	-0.057725	4.815458
281.595732	8000.107456	11.017715	-0.057725	4.815462
281.530511	8000.094632	11.022720	-0.057713	4.815459
281.559131	8000.089769	11.027725	-0.057718	4.815457
281.689088	8000.159243	11.032730	-0.057743	4.815477
281.635210	8000.146607	11.037735	-0.057733	4.815473
281.622432	8000.158158	11.042739	-0.057731	4.815477
281.659098	8000.114958	11.047744	-0.057737	4.815464
281.634471	8000.098530	11.052749	-0.057733	4.815459
281.623702	8000.134692	11.057754	-0.057731	4.815470
281.680562	8000.085413	11.062759	-0.057742	4.815455
281.792963	8000.133226	11.067763	-0.057763	4.815469
281.668811	8000.176066	11.072768	-0.057740	4.815482
281.584047	8000.103078	11.077773	-0.057724	4.815461
281.733247	8000.116233	11.082778	-0.057752	4.815464
281.659939	8000.093659	11.087783	-0.057738	4.815458
281.488086	8000.134644	11.092787	-0.057706	4.815471
281.476565	8000.131255	11.097792	-0.057704	4.815470
281.516913	8000.083841	11.102797	-0.057712	4.815456
281.592706	8000.081893	11.107802	-0.057726	4.815455
281.351548	8000.103568	11.112807	-0.057681	4.815462
281.441768	8000.126436	11.117811	-0.057698	4.815468
281.483246	8000.077972	11.122816	-0.057706	4.815454
281.446168	8000.093397	11.127821	-0.057699	4.815459
281.387205	8000.134107	11.132826	-0.057688	4.815471
281.492529	8000.108069	11.137831	-0.057708	4.815463
281.503518	8000.110395	11.142835	-0.057710	4.815464
281.576916	8000.096653	11.147840	-0.057724	4.815459
281.712329	8000.089277	11.152845	-0.057749	4.815456
281.539668	8000.151621	11.157850	-0.057717	4.815475
281.481689	8000.083349	11.162855	-0.057706	4.815456
281.726537	8000.134416	11.167859	-0.057752	4.815469
281.817270	8000.130577	11.172864	-0.057769	4.815468
281.585965	8000.106464	11.177869	-0.057726	4.815462
281.648925	8000.118197	11.182874	-0.057738	4.815465
281.749429	8000.092079	11.187879	-0.057757	4.815457
281.794613	8000.115272	11.192883	-0.057765	4.815464
281.518189	8000.092552	11.197888	-0.057714	4.815458
281.641193	8000.097795	11.202893	-0.057737	4.815459
281.677275	8000.131525	11.207898	-0.057744	4.815469
281.627263	8000.099717	11.212903	-0.057734	4.815460
281.633530	8000.104103	11.217907	-0.057736	4.815461
281.640653	8000.110639	11.222912	-0.057737	4.815463
281.445710	8000.079646	11.227917	-0.057701	4.815455
281.536581	8000.103594	11.232922	-0.057718	4.815461
281.541646	8000.084450	11.237927	-0.057719	4.815456
281.687751	8000.113583	11.242931	-0.057746	4.815464
281.640947	8000.138465	11.247936	-0.057737	4.815471
281.534949	8000.099322	11.252941	-0.057718	4.815460
281.606718	8000.101583	11.257946	-0.057731	4.815460
281.670532	8000.079134	11.262951	-0.057743	4.815454
281.733312	8000.097275	11.267955	-0.057755	4.815459
281.817889	8000.070894	11.272960	-0.057771	4.815450
281.887428	8000.089147	11.277965	-0.057784	4.815455
281.726537	8000.104666	11.282970	-0.057754	4.815461
281.737810	8000.085624	11.287975	-0.057756	4.815455
281.742277	8000.102803	11.292979	-0.057757	4.815460
281.645942	8000.079849	11.297984	-0.057739	4.815454
281.729590	8000.116500	11.302989	-0.057755	4.815464
281.920260	8000.175223	11.307994	-0.057790	4.815480
281.761205	8000.099939	11.312999	-0.057761	4.815459
281.789743	8000.118584	11.318003	-0.057766	4.815464
281.926204	8000.118706	11.323008	-0.057792	4.815464
281.754534	8000.114812	11.328013	-0.057760	4.815464
281.723856	8000.135686	11.333018	-0.057754	4.815470
281.620216	8000.119022	11.338023	-0.057735	4.815465
281.575148	8000.141795	11.343027	-0.057727	4.815472
281.669686	8000.128402	11.348032	-0.057744	4.815468
281.678853	8000.082611	11.353037	-0.057746	4.815454
281.675161	8000.072940	11.358042	-0.057746	4.815452
281.640344	8000.086265	11.363047	-0.057739	4.815456
281.670199	8000.140195	11.368051	-0.057745	4.815471
281.882806	8000.151192	11.373056	-0.057785	4.815473
281.644754	8000.108800	11.378061	-0.057740	4.815462
281.702635	8000.126861	11.383066	-0.057751	4.815467
281.783305	8000.094004	11.388071	-0.057766	4.815457
281.939391	8000.123302	11.393075	-0.057795	4.815465
281.644229	8000.132331	11.398080	-0.057741	4.815469
281.636350	8000.106562	11.403085	-0.057739	4.815462
281.612097	8000.147845	11.408090	-0.057735	4.815474
281.659676	8000.085589	11.413095	-0.057744	4.815455
281.566900	8000.116124	11.418099	-0.057726	4.815465
281.683818	8000.108443	11.423104	-0.057748	4.815462
281.594073	8000.088804	11.428109	-0.057732	4.815457
281.564008	8000.091521	11.433114	-0.057726	4.815458
281.455271	8000.064088	11.438119	-0.057706	4.815450
281.752374	8000.088232	11.443123	-0.057761	4.815456
281.771489	8000.104584	11.448128	-0.057765	4.815460
281.671725	8000.110426	11.453133	-0.057747	4.815463
281.877159	8000.150156	11.458138	-0.057785	4.815473
281.615009	8000.106299	11.463143	-0.057736	4.815462
281.775639	8000.132467	11.468147	-0.057766	4.815468
281.637138	8000.128051	11.473152	-0.057740	4.815468
281.828983	8000.105578	11.478157	-0.057776	4.815460
281.645210	8000.094004	11.483162	-0.057742	4.815458
281.710734	8000.091887	11.488167	-0.057754	4.815457
281.976652	8000.141164	11.493171	-0.057804	4.815470
281.672610	8000.097684	11.498176	-0.057747	4.815459
281.485981	8000.086063	11.503181	-0.057713	4.815456
281.785031	8000.123064	11.508186	-0.057769	4.815466
282.064014	8000.077450	11.513191	-0.057821	4.815451
281.934963	8000.105249	11.518195	-0.057797	4.815460
281.957060	8000.107758	11.523200	-0.057801	4.815460
281.648418	8000.113359	11.528205	-0.057743	4.815464
281.827022	8000.146235	11.533210	-0.057777	4.815472
281.741911	8000.120259	11.538215	-0.057761	4.815465
281.911368	8000.116652	11.543219	-0.057793	4.815463
281.787130	8000.131707	11.548224	-0.057770	4.815468
281.875404	8000.104318	11.553229	-0.057786	4.815460
282.071477	8000.123591	11.558234	-0.057823	4.815464
281.758064	8000.107740	11.563239	-0.057764	4.815461
281.599055	8000.116878	11.568243	-0.057735	4.815465
281.664773	8000.104078	11.573248	-0.057747	4.815461
281.709396	8000.063146	11.578253	-0.057756	4.815449
281.698818	8000.104655	11.583258	-0.057754	4.815461
281.845222	8000.093186	11.588263	-0.057781	4.815457
281.905260	8000.139066	11.593267	-0.057792	4.815470
281.940197	8000.155680	11.598272	-0.057799	4.815474
281.774593	8000.102729	11.603277	-0.057768	4.815460
281.876426	8000.116172	11.608282	-0.057787	4.815463
281.688110	8000.092768	11.613287	-0.057752	4.815457
281.845203	8000.103917	11.618291	-0.057782	4.815460
281.853378	8000.079481	11.623296	-0.057783	4.815453
281.914909	8000.087984	11.628301	-0.057795	4.815455
281.976735	8000.161678	11.633306	-0.057806	4.815476
281.847598	8000.094368	11.638311	-0.057782	4.815457
281.872456	8000.108678	11.643315	-0.057787	4.815461
281.957763	8000.113299	11.648320	-0.057803	4.815462
281.772422	8000.108111	11.653325	-0.057769	4.815461
281.791147	8000.138348	11.658330	-0.057772	4.815470
281.679932	8000.100188	11.663335	-0.057752	4.815459
281.688088	8000.103536	11.668339	-0.057753	4.815460
281.803479	8000.075526	11.673344	-0.057775	4.815452
281.816164	8000.094978	11.678349	-0.057777	4.815457
281.825313	8000.114371	11.683354	-0.057779	4.815463
281.722896	8000.077424	11.688359	-0.057760	4.815453
281.920538	8000.112752	11.693363	-0.057797	4.815462
282.084004	8000.144310	11.698368	-0.057827	4.815470
281.939392	8000.104529	11.703373	-0.057801	4.815459
282.000035	8000.134390	11.708378	-0.057812	4.815468
281.793486	8000.080764	11.713383	-0.057774	4.815453
281.769118	8000.095330	11.718387	-0.057769	4.815458
281.871362	8000.148318	11.723392	-0.057788	4.815473
281.841207	8000.124318	11.728397	-0.057783	4.815466
281.805589	8000.104503	11.733402	-0.057776	4.815460
281.798757	8000.071270	11.738407	-0.057775	4.815450
281.942179	8000.118526	11.743411	-0.057802	4.815464
282.134331	8000.105676	11.748416	-0.057838	4.815459
281.870725	8000.081029	11.753421	-0.057789	4.815453
281.890670	8000.151895	11.758426	-0.057792	4.815473
281.895563	8000.099620	11.763431	-0.057793	4.815458
282.074033	8000.118603	11.768435	-0.057827	4.815463
282.112379	8000.149164	11.773440	-0.057834	4.815472
282.000655	8000.099240	11.778445	-0.057813	4.815458
282.002929	8000.121726	11.783450	-0.057814	4.815464
281.998286	8000.121657	11.788455	-0.057813	4.815464
282.172927	8000.134164	11.793459	-0.057846	4.815467
282.260819	8000.133485	11.798464	-0.057862	4.815466
282.036030	8000.096655	11.803469	-0.057820	4.815457
282.061158	8000.101352	11.808474	-0.057825	4.815458
282.116248	8000.078759	11.813479	-0.057835	4.815451
281.972830	8000.102046	11.818483	-0.057809	4.815459
282.005780	8000.147479	11.823488	-0.057815	4.815472
281.785391	8000.103242	11.828493	-0.057774	4.815460
281.951919	8000.143399	11.833498	-0.057805	4.815471
282.013172	8000.111291	11.838503	-0.057817	4.815461
282.025857	8000.100821	11.843507	-0.057819	4.815458
281.948294	8000.111303	11.848512	-0.057805	4.815461
281.791609	8000.092696	11.853517	-0.057776	4.815457
281.924496	8000.125886	11.858522	-0.057800	4.815466
281.864263	8000.080018	11.863527	-0.057789	4.815453
281.869007	8000.077966	11.868531	-0.057790	4.815452
281.918794	8000.080932	11.873536	-0.057800	4.815453
281.971283	8000.075394	11.878541	-0.057809	4.815451
282.025373	8000.113696	11.883546	-0.057820	4.815462
281.838266	8000.149086	11.888551	-0.057785	4.815473
281.925773	8000.153744	11.893555	-0.057801	4.815474
282.134286	8000.144369	11.898560	-0.057840	4.815470
281.954859	8000.104013	11.903565	-0.057807	4.815459
281.925857	8000.139875	11.908570	-0.057802	4.815470
281.754842	8000.098590	11.913575	-0.057770	4.815459
281.914637	8000.123676	11.918579	-0.057800	4.815465
282.055832	8000.111053	11.923584	-0.057826	4.815461
282.049797	8000.074627	11.928589	-0.057825	4.815450
282.224726	8000.109581	11.933594	-0.057858	4.815459
282.057735	8000.086528	11.938599	-0.057827	4.815454
281.965393	8000.112796	11.943603	-0.057809	4.815462
282.127826	8000.117621	11.948608	-0.057840	4.815462
281.918418	8000.079977	11.953613	-0.057801	4.815452
281.941768	8000.106016	11.958618	-0.057805	4.815460
281.998490	8000.081313	11.963623	-0.057816	4.815452
281.935687	8000.096313	11.968627	-0.057804	4.815457
281.941272	8000.078246	11.973632	-0.057805	4.815452
281.986692	8000.086484	11.978637	-0.057814	4.815454
281.945175	8000.112522	11.983642	-0.057806	4.815462
281.998162	8000.121952	11.988647	-0.057816	4.815464
281.973430	8000.113003	11.993651	-0.057812	4.815462
281.914235	8000.107759	11.998656	-0.057801	4.815460
281.969029	8000.087298	12.003661	-0.057811	4.815454
281.900878	8000.103279	12.008666	-0.057799	4.815459
281.958733	8000.083937	12.013671	-0.057809	4.815453
281.971796	8000.100190	12.018675	-0.057812	4.815458
281.912065	8000.083182	12.023680	-0.057801	4.815453
281.904930	8000.084140	12.028685	-0.057800	4.815454
282.180347	8000.114340	12.033690	-0.057851	4.815461
282.247615	8000.093017	12.038695	-0.057864	4.815454
282.022092	8000.101057	12.043699	-0.057822	4.815458
282.022995	8000.125657	12.048704	-0.057822	4.815465
281.913876	8000.109972	12.053709	-0.057802	4.815461
282.095568	8000.136488	12.058714	-0.057836	4.815468
282.110528	8000.097203	12.063719	-0.057839	4.815456
282.120387	8000.115540	12.068723	-0.057840	4.815462
282.040698	8000.149497	12.073728	-0.057826	4.815472
281.923222	8000.118712	12.078733	-0.057804	4.815464
282.030624	8000.127973	12.083738	-0.057824	4.815466
281.934606	8000.096474	12.088743	-0.057806	4.815457
281.901525	8000.107690	12.093747	-0.057800	4.815460
282.184696	8000.130538	12.098752	-0.057853	4.815466
282.170626	8000.114284	12.103757	-0.057850	4.815461
281.984455	8000.106944	12.108762	-0.057816	4.815460
282.093682	8000.088450	12.113767	-0.057836	4.815454
282.114720	8000.109109	12.118771	-0.057840	4.815460
282.151716	8000.114002	12.123776	-0.057847	4.815461
282.128193	8000.096523	12.128781	-0.057843	4.815456
282.402318	8000.136320	12.133786	-0.057894	4.815466
282.310893	8000.087798	12.138791	-0.057877	4.815453
282.050232	8000.119837	12.143795	-0.057829	4.815463
282.248817	8000.110298	12.148800	-0.057866	4.815459
282.041658	8000.081240	12.153805	-0.057827	4.815452
282.151975	8000.140774	12.158810	-0.057848	4.815469
281.939764	8000.088122	12.163815	-0.057808	4.815454
282.257189	8000.114741	12.168819	-0.057868	4.815461
282.360911	8000.112186	12.173824	-0.057887	4.815459
282.208537	8000.111815	12.178829	-0.057859	4.815460
282.360346	8000.143182	12.183834	-0.057887	4.815468
282.111392	8000.116639	12.188839	-0.057841	4.815462
282.074740	8000.085051	12.193843	-0.057834	4.815453
282.263049	8000.099921	12.198848	-0.057869	4.815456
282.147092	8000.084123	12.203853	-0.057848	4.815452
282.338057	8000.140714	12.208858	-0.057883	4.815468
282.055182	8000.090101	12.213863	-0.057831	4.815454
282.160873	8000.123912	12.218867	-0.057851	4.815464
282.106213	8000.117674	12.223872	-0.057840	4.815462
281.894683	8000.079994	12.228877	-0.057801	4.815452
282.062057	8000.095588	12.233882	-0.057832	4.815456
282.014825	8000.100159	12.238887	-0.057824	4.815458
282.042517	8000.105966	12.243891	-0.057829	4.815459
282.012280	8000.105475	12.248896	-0.057823	4.815459
282.002264	8000.091425	12.253901	-0.057822	4.815455
282.260649	8000.122412	12.258906	-0.057870	4.815463
282.316925	8000.097702	12.263911	-0.057880	4.815455
282.371049	8000.103945	12.268915	-0.057890	4.815457
282.404261	8000.126942	12.273920	-0.057897	4.815464
282.289188	8000.120776	12.278925	-0.057875	4.815462
282.376518	8000.153215	12.283930	-0.057892	4.815471
282.340679	8000.114160	12.288935	-0.057885	4.815460
282.230931	8000.120905	12.293939	-0.057865	4.815463
282.108399	8000.149880	12.298944	-0.057842	4.815472
282.152928	8000.083299	12.303949	-0.057850	4.815452
282.018847	8000.111015	12.308954	-0.057826	4.815461
282.039331	8000.125253	12.313959	-0.057829	4.815465
282.083385	8000.097135	12.318963	-0.057838	4.815456
282.099374	8000.108092	12.323968	-0.057841	4.815459
282.066038	8000.102206	12.328973	-0.057835	4.815458
282.246256	8000.123355	12.333978	-0.057868	4.815463
282.305223	8000.130748	12.338983	-0.057879	4.815465
282.173582	8000.127513	12.343987	-0.057855	4.815465
282.162330	8000.099551	12.348992	-0.057853	4.815457
282.262463	8000.104417	12.353997	-0.057872	4.815458
282.297715	8000.143477	12.359002	-0.057878	4.815469
282.159847	8000.115562	12.364007	-0.057853	4.815461
282.157494	8000.119805	12.369011	-0.057852	4.815463
282.257643	8000.120397	12.374016	-0.057871	4.815462
282.248333	8000.091397	12.379021	-0.057869	4.815454
282.421227	8000.176543	12.384026	-0.057902	4.815478
282.440595	8000.135194	12.389031	-0.057905	4.815466
282.256759	8000.134304	12.394035	-0.057871	4.815466
282.135530	8000.113075	12.399040	-0.057849	4.815461
282.244862	8000.094583	12.404045	-0.057869	4.815455
282.298069	8000.145695	12.409050	-0.057879	4.815469
282.073213	8000.083216	12.414055	-0.057837	4.815452
282.077174	8000.117485	12.419059	-0.057838	4.815462
282.276530	8000.172077	12.424064	-0.057876	4.815477
282.044660	8000.107346	12.429069	-0.057832	4.815459
282.123402	8000.131094	12.434074	-0.057847	4.815466
282.033567	8000.099697	12.439079	-0.057830	4.815457
282.210509	8000.105831	12.444083	-0.057864	4.815458
282.336525	8000.118604	12.449088	-0.057887	4.815461
282.124228	8000.098010	12.454093	-0.057848	4.815456
282.240267	8000.117031	12.459098	-0.057869	4.815461
282.253865	8000.085204	12.464103	-0.057872	4.815452
282.222131	8000.108197	12.469107	-0.057866	4.815459
282.187197	8000.117246	12.474112	-0.057860	4.815462
282.058700	8000.061701	12.479117	-0.057836	4.815446
282.067792	8000.104603	12.484122	-0.057838	4.815459
282.310897	8000.129996	12.489127	-0.057883	4.815465
282.393059	8000.119605	12.494131	-0.057898	4.815461
282.280796	8000.148749	12.499136	-0.057878	4.815470
282.272920	8000.091989	12.504141	-0.057876	4.815454
282.429078	8000.115947	12.509146	-0.057905	4.815460
282.425689	8000.109487	12.514151	-0.057905	4.815458
282.298093	8000.118074	12.519155	-0.057881	4.815461
282.386027	8000.135563	12.524160	-0.057898	4.815466
282.344589	8000.086798	12.529165	-0.057890	4.815452
282.583285	8000.106775	12.534170	-0.057934	4.815457
282.506159	8000.126882	12.539175	-0.057920	4.815463
282.292350	8000.134046	12.544179	-0.057880	4.815466
282.184907	8000.118388	12.549184	-0.057861	4.815462
282.042874	8000.090404	12.554189	-0.057834	4.815454
282.112559	8000.171709	12.559194	-0.057847	4.815478
282.087794	8000.164896	12.564199	-0.057843	4.815476
282.064832	8000.121779	12.569203	-0.057839	4.815464
282.312708	8000.161143	12.574208	-0.057885	4.815474
282.235186	8000.100027	12.579213	-0.057870	4.815456
282.222755	8000.124408	12.584218	-0.057868	4.815464
282.270832	8000.099562	12.589223	-0.057877	4.815456
282.371482	8000.129015	12.594227	-0.057896	4.815464
282.319128	8000.145256	12.599232	-0.057886	4.815469
282.421806	8000.119174	12.604237	-0.057906	4.815461
282.589916	8000.156153	12.609242	-0.057937	4.815471
282.473608	8000.136074	12.614247	-0.057915	4.815466
282.328689	8000.153993	12.619251	-0.057888	4.815472
282.529568	8000.222504	12.624256	-0.057926	4.815491
282.301927	8000.154635	12.629261	-0.057884	4.815472
282.274995	8000.168090	12.634266	-0.057879	4.815476
282.120169	8000.134552	12.639271	-0.057850	4.815467
282.387787	8000.140045	12.644275	-0.057900	4.815467
282.367901	8000.146136	12.649280	-0.057896	4.815469
282.215273	8000.128663	12.654285	-0.057868	4.815465
282.303345	8000.166458	12.659290	-0.057884	4.815475
282.228772	8000.160960	12.664295	-0.057871	4.815474
282.303135	8000.133342	12.669299	-0.057885	4.815466
282.429753	8000.138645	12.674304	-0.057908	4.815467
282.248668	8000.107879	12.679309	-0.057875	4.815459
282.336586	8000.114681	12.684314	-0.057891	4.815460
282.472336	8000.145782	12.689319	-0.057916	4.815468
282.432743	8000.138724	12.694323	-0.057909	4.815467
282.466625	8000.187380	12.699328	-0.057916	4.815481
282.188237	8000.104782	12.704333	-0.057864	4.815458
282.263659	8000.133818	12.709338	-0.057878	4.815466
282.330788	8000.144552	12.714343	-0.057890	4.815469
282.274856	8000.105165	12.719347	-0.057880	4.815458
282.575234	8000.151808	12.724352	-0.057936	4.815470
282.393580	8000.133855	12.729357	-0.057902	4.815465
282.406366	8000.176819	12.734362	-0.057905	4.815478
282.362260	8000.126942	12.739367	-0.057897	4.815464
282.201985	8000.108274	12.744371	-0.057867	4.815459
282.366537	8000.121684	12.749376	-0.057898	4.815462
282.454485	8000.090015	12.754381	-0.057914	4.815452
282.402557	8000.134048	12.759386	-0.057905	4.815465
282.445799	8000.105916	12.764391	-0.057913	4.815457
282.490182	8000.095970	12.769395	-0.057921	4.815454
282.406567	8000.136274	12.774400	-0.057906	4.815466
282.628912	8000.119648	12.779405	-0.057947	4.815460
282.611991	8000.154641	12.784410	-0.057944	4.815470
282.587652	8000.130737	12.789415	-0.057940	4.815464
282.468799	8000.126645	12.794419	-0.057918	4.815463
282.476720	8000.197313	12.799424	-0.057919	4.815483
282.491807	8000.166579	12.804429	-0.057922	4.815474
282.367801	8000.152784	12.809434	-0.057899	4.815471
282.354438	8000.144022	12.814439	-0.057897	4.815468
282.343909	8000.126758	12.819443	-0.057895	4.815464
282.399152	8000.165079	12.824448	-0.057905	4.815474
282.267620	8000.108415	12.829453	-0.057881	4.815459
282.335591	8000.110613	12.834458	-0.057893	4.815459
282.513331	8000.106074	12.839463	-0.057927	4.815457
282.616788	8000.134506	12.844467	-0.057946	4.815464
282.724810	8000.183317	12.849472	-0.057966	4.815478
282.661861	8000.157706	12.854477	-0.057954	4.815471
282.368043	8000.172098	12.859482	-0.057900	4.815477
282.301527	8000.125057	12.864487	-0.057888	4.815463
282.486243	8000.140937	12.869491	-0.057922	4.815467
282.616506	8000.152712	12.874496	-0.057946	4.815470
282.537667	8000.131114	12.879501	-0.057932	4.815464
282.335384	8000.153430	12.884506	-0.057894	4.815471
282.481448	8000.141956	12.889511	-0.057921	4.815467
282.545516	8000.144090	12.894515	-0.057933	4.815468
282.356377	8000.153799	12.899520	-0.057898	4.815471
282.349197	8000.122697	12.904525	-0.057897	4.815462
282.522300	8000.140523	12.909530	-0.057929	4.815467
282.742486	8000.149509	12.914535	-0.057971	4.815468
282.347193	8000.129098	12.919539	-0.057897	4.815464
282.486120	8000.180556	12.924544	-0.057923	4.815478
282.694057	8000.148732	12.929549	-0.057962	4.815468
282.509094	8000.147823	12.934554	-0.057927	4.815469
282.374123	8000.153082	12.939559	-0.057902	4.815471
282.144180	8000.158912	12.944563	-0.057860	4.815474
282.467986	8000.166402	12.949568	-0.057920	4.815474
282.321510	8000.142619	12.954573	-0.057893	4.815468
282.213988	8000.134439	12.959578	-0.057873	4.815466
282.250093	8000.124356	12.964583	-0.057880	4.815463
282.206496	8000.123644	12.969587	-0.057872	4.815463
282.491961	8000.172178	12.974592	-0.057925	4.815476
282.468632	8000.129055	12.979597	-0.057921	4.815464
282.475333	8000.151614	12.984602	-0.057922	4.815470
282.344616	8000.146258	12.989607	-0.057898	4.815469
282.389085	8000.111735	12.994611	-0.057906	4.815459
282.411403	8000.118522	12.999616	-0.057910	4.815461
282.283748	8000.121766	13.004621	-0.057887	4.815462
282.593445	8000.163219	13.009626	-0.057944	4.815473
282.631218	8000.132860	13.014631	-0.057951	4.815464
282.561675	8000.119964	13.019635	-0.057939	4.815460
282.513924	8000.160860	13.024640	-0.057930	4.815473
282.539531	8000.103584	13.029645	-0.057935	4.815456
282.437814	8000.166030	13.034650	-0.057916	4.815474
282.378701	8000.129797	13.039655	-0.057905	4.815464
282.550000	8000.131564	13.044659	-0.057937	4.815464
282.588526	8000.110834	13.049664	-0.057944	4.815458
282.448330	8000.126694	13.054669	-0.057918	4.815463
282.348481	8000.149632	13.059674	-0.057900	4.815470
282.371476	8000.135058	13.064679	-0.057904	4.815466
282.405837	8000.106780	13.069683	-0.057910	4.815457
282.572708	8000.138395	13.074688	-0.057942	4.815466
282.648658	8000.128970	13.079693	-0.057956	4.815463
282.586607	8000.131159	13.084698	-0.057944	4.815464
282.451759	8000.131077	13.089703	-0.057919	4.815464
282.372531	8000.123365	13.094707	-0.057905	4.815462
282.589057	8000.130153	13.099712	-0.057945	4.815463
282.442899	8000.120267	13.104717	-0.057918	4.815461
282.435206	8000.123354	13.109722	-0.057917	4.815462
282.703370	8000.159847	13.114727	-0.057967	4.815471
282.393620	8000.107721	13.119731	-0.057909	4.815458
282.394341	8000.139799	13.124736	-0.057909	4.815467
282.418013	8000.148747	13.129741	-0.057914	4.815469
282.557270	8000.143573	13.134746	-0.057940	4.815467
282.506951	8000.169465	13.139751	-0.057930	4.815475
282.263214	8000.134459	13.144755	-0.057885	4.815466
282.520278	8000.146190	13.149760	-0.057933	4.815468
282.597844	8000.131449	13.154765	-0.057948	4.815464
282.536823	8000.131517	13.159770	-0.057936	4.815464
282.433092	8000.125538	13.164775	-0.057917	4.815463
282.457031	8000.118460	13.169779	-0.057922	4.815460
282.614756	8000.188396	13.174784	-0.057951	4.815480
282.416055	8000.108181	13.179789	-0.057914	4.815458
282.514463	8000.134391	13.184794	-0.057933	4.815465
282.507017	8000.126795	13.189799	-0.057931	4.815463
282.673519	8000.114591	13.194803	-0.057962	4.815458
282.727991	8000.141145	13.199808	-0.057973	4.815466
282.624328	8000.115931	13.204813	-0.057953	4.815459
282.554388	8000.156460	13.209818	-0.057940	4.815471
282.683694	8000.142573	13.214823	-0.057965	4.815466
282.769161	8000.131168	13.219827	-0.057981	4.815463
282.531434	8000.137937	13.224832	-0.057936	4.815466
282.403019	8000.118726	13.229837	-0.057913	4.815461
282.530648	8000.127253	13.234842	-0.057936	4.815463
282.654534	8000.134648	13.239847	-0.057960	4.815464
282.617804	8000.118020	13.244851	-0.057953	4.815459
282.755138	8000.183345	13.249856	-0.057979	4.815478
282.498407	8000.133162	13.254861	-0.057931	4.815464
282.413710	8000.138183	13.259866	-0.057915	4.815466
282.462509	8000.116555	13.264871	-0.057924	4.815460
282.462754	8000.112292	13.269875	-0.057924	4.815459
282.640498	8000.151567	13.274880	-0.057958	4.815469
282.481324	8000.095515	13.279885	-0.057928	4.815454
282.617246	8000.129825	13.284890	-0.057953	4.815463
282.531150	8000.167951	13.289895	-0.057937	4.815474
282.423790	8000.113823	13.294899	-0.057918	4.815459
282.571486	8000.145122	13.299904	-0.057945	4.815468
282.632399	8000.127968	13.304909	-0.057957	4.815462
282.596997	8000.143421	13.309914	-0.057950	4.815467
282.474001	8000.147809	13.314919	-0.057927	4.815469
282.423136	8000.120261	13.319923	-0.057918	4.815461
282.497331	8000.200573	13.324928	-0.057932	4.815484
282.308798	8000.119457	13.329933	-0.057897	4.815461
282.493237	8000.117166	13.334938	-0.057931	4.815460
282.516636	8000.136795	13.339943	-0.057936	4.815465
282.412378	8000.109434	13.344947	-0.057916	4.815458
282.617063	8000.190832	13.349952	-0.057954	4.815481
282.615867	8000.119220	13.354957	-0.057954	4.815460
282.625008	8000.125791	13.359962	-0.057956	4.815462
282.561071	8000.135429	13.364967	-0.057944	4.815465
282.501808	8000.104536	13.369971	-0.057933	4.815456
282.452616	8000.145408	13.374976	-0.057924	4.815468
282.440316	8000.109948	13.379981	-0.057922	4.815458
282.450370	8000.110121	13.384986	-0.057924	4.815458
282.495685	8000.148279	13.389991	-0.057933	4.815469
282.460706	8000.102826	13.394995	-0.057926	4.815456
282.602609	8000.142579	13.400000	-0.057953	4.815467
282.686643	8000.091610	13.405005	-0.057968	4.815451
282.675114	8000.135241	13.410010	-0.057966	4.815464
282.732932	8000.126586	13.415015	-0.057977	4.815461
282.411125	8000.128761	13.420019	-0.057917	4.815464
282.572555	8000.210513	13.425024	-0.057947	4.815487
282.661154	8000.112599	13.430029	-0.057964	4.815458
282.570216	8000.134615	13.435034	-0.057947	4.815464
282.527300	8000.089032	13.440039	-0.057939	4.815451
282.402706	8000.100875	13.445043	-0.057916	4.815455
282.513655	8000.136910	13.450048	-0.057937	4.815465
282.442551	8000.105822	13.455053	-0.057924	4.815457
282.502880	8000.113237	13.460058	-0.057935	4.815459
282.524311	8000.081539	13.465063	-0.057939	4.815449
282.482031	8000.086192	13.470067	-0.057931	4.815451
282.703340	8000.156108	13.475072	-0.057973	4.815470
282.613404	8000.116160	13.480077	-0.057956	4.815459
282.598208	8000.152250	13.485082	-0.057953	4.815469
282.581747	8000.175496	13.490087	-0.057950	4.815476
282.505276	8000.120809	13.495091	-0.057936	4.815461
282.668230	8000.126713	13.500096	-0.057966	4.815462
282.633869	8000.114398	13.505101	-0.057960	4.815458
282.801107	8000.153500	13.510106	-0.057991	4.815469
282.764688	8000.152906	13.515111	-0.057985	4.815469
282.541815	8000.100077	13.520115	-0.057943	4.815454
282.769628	8000.145522	13.525120	-0.057986	4.815467
282.510075	8000.085675	13.530125	-0.057938	4.815450
282.481713	8000.125823	13.535130	-0.057932	4.815462
282.670141	8000.113980	13.540135	-0.057968	4.815458
282.692249	8000.113284	13.545139	-0.057972	4.815458
282.709066	8000.179825	13.550144	-0.057975	4.815477
282.540738	8000.149268	13.555149	-0.057944	4.815469
282.694882	8000.164645	13.560154	-0.057972	4.815473
282.789679	8000.144844	13.565159	-0.057990	4.815466
282.625546	8000.113288	13.570163	-0.057960	4.815458
282.823559	8000.162517	13.575168	-0.057997	4.815471
282.584799	8000.112631	13.580173	-0.057952	4.815458
282.644264	8000.142473	13.585178	-0.057963	4.815466
282.893663	8000.180795	13.590183	-0.058010	4.815476
282.761139	8000.145486	13.595187	-0.057985	4.815467
282.763667	8000.162634	13.600192	-0.057986	4.815472
282.951825	8000.137963	13.605197	-0.058021	4.815464
282.638610	8000.147760	13.610202	-0.057963	4.815468
282.784087	8000.146964	13.615207	-0.057990	4.815467
282.596048	8000.096846	13.620211	-0.057955	4.815453
282.784000	8000.145908	13.625216	-0.057990	4.815467
282.521285	8000.098833	13.630221	-0.057941	4.815454
282.623051	8000.131511	13.635226	-0.057960	4.815463
282.778673	8000.098823	13.640231	-0.057989	4.815453
282.811099	8000.106846	13.645235	-0.057996	4.815455
282.730590	8000.127966	13.650240	-0.057981	4.815462
282.799942	8000.147285	13.655245	-0.057994	4.815467
283.006368	8000.150701	13.660250	-0.058032	4.815467
282.776343	8000.172558	13.665255	-0.057989	4.815474
282.529765	8000.118268	13.670259	-0.057944	4.815460
282.879509	8000.155040	13.675264	-0.058009	4.815469
282.842910	8000.130933	13.680269	-0.058002	4.815462
282.803205	8000.133491	13.685274	-0.057995	4.815463
282.814775	8000.172161	13.690279	-0.057997	4.815474
282.642689	8000.122307	13.695283	-0.057965	4.815460
282.533653	8000.127995	13.700288	-0.057945	4.815463
282.644516	8000.151205	13.705293	-0.057966	4.815469
282.787107	8000.143949	13.710298	-0.057992	4.815466
282.822163	8000.156291	13.715303	-0.057999	4.815469
282.490349	8000.128378	13.720307	-0.057937	4.815463
282.729947	8000.152645	13.725312	-0.057982	4.815469
282.500255	8000.101841	13.730317	-0.057939	4.815455
282.457013	8000.134262	13.735322	-0.057931	4.815465
282.593003	8000.149338	13.740327	-0.057957	4.815468
282.791954	8000.124846	13.745331	-0.057994	4.815460
282.736842	8000.165620	13.750336	-0.057983	4.815473
282.727135	8000.122722	13.755341	-0.057982	4.815460
282.835674	8000.151237	13.760346	-0.058002	4.815468
282.610728	8000.144325	13.765351	-0.057960	4.815467
282.637656	8000.128747	13.770355	-0.057965	4.815462
282.781273	8000.157842	13.775360	-0.057992	4.815470
282.925720	8000.159166	13.780365	-0.058019	4.815470
282.888526	8000.155353	13.785370	-0.058012	4.815469
282.821984	8000.168154	13.790375	-0.058000	4.815473
282.811668	8000.127383	13.795379	-0.057998	4.815461
282.780612	8000.166418	13.800384	-0.057992	4.815473
282.881643	8000.139240	13.805389	-0.058011	4.815464
282.823290	8000.147901	13.810394	-0.058001	4.815467
282.809291	8000.163707	13.815399	-0.057998	4.815472
282.834962	8000.125667	13.820403	-0.058003	4.815460
283.142496	8000.171362	13.825408	-0.058060	4.815472
283.098532	8000.208046	13.830413	-0.058052	4.815483
282.718901	8000.166519	13.835418	-0.057982	4.815473
282.766824	8000.163043	13.840423	-0.057991	4.815472
282.817041	8000.132889	13.845427	-0.058000	4.815463
282.941175	8000.159525	13.850432	-0.058023	4.815470
282.877668	8000.195887	13.855437	-0.058011	4.815481
282.938963	8000.144543	13.860442	-0.058023	4.815465
282.930147	8000.168983	13.865447	-0.058021	4.815473
282.745521	8000.154187	13.870451	-0.057987	4.815469
282.642371	8000.169590	13.875456	-0.057968	4.815474
282.725028	8000.137834	13.880461	-0.057983	4.815464
282.566251	8000.163005	13.885466	-0.057954	4.815473
282.647399	8000.255187	13.890471	-0.057969	4.815499
282.541315	8000.203217	13.895475	-0.057950	4.815484
282.532919	8000.220184	13.900480	-0.057948	4.815489
282.543062	8000.224633	13.905485	-0.057950	4.815491
282.800216	8000.173317	13.910490	-0.057998	4.815474
282.919720	8000.167817	13.915495	-0.058020	4.815472
282.665919	8000.148673	13.920499	-0.057973	4.815468
282.953532	8000.189763	13.925504	-0.058027	4.815478
282.909093	8000.227509	13.930509	-0.058019	4.815490
282.755050	8000.157647	13.935514	-0.057990	4.815470
282.687711	8000.151200	13.940519	-0.057978	4.815468
282.620858	8000.140486	13.945523	-0.057965	4.815466
282.616987	8000.189587	13.950528	-0.057965	4.815480
282.566758	8000.152431	13.955533	-0.057955	4.815469
282.551614	8000.151120	13.960538	-0.057953	4.815469
282.784884	8000.172077	13.965543	-0.057996	4.815474
282.576123	8000.136578	13.970547	-0.057957	4.815465
282.818446	8000.190813	13.975552	-0.058002	4.815479
282.921783	8000.171154	13.980557	-0.058022	4.815473
282.665153	8000.159443	13.985562	-0.057974	4.815471
282.794249	8000.175475	13.990567	-0.057998	4.815475
282.742070	8000.134012	13.995571	-0.057989	4.815463
282.684940	8000.174754	14.000576	-0.057978	4.815475
282.672510	8000.169213	14.005581	-0.057976	4.815474
282.784615	8000.189238	14.010586	-0.057997	4.815479
282.745865	8000.233489	14.015591	-0.057990	4.815492
282.634552	8000.110901	14.020595	-0.057969	4.815457
282.802457	8000.161770	14.025600	-0.058000	4.815471
282.771022	8000.121719	14.030605	-0.057995	4.815459
282.930608	8000.116880	14.035610	-0.058024	4.815457
282.758953	8000.153594	14.040615	-0.057992	4.815469
282.738753	8000.137238	14.045619	-0.057989	4.815464
282.797065	8000.167062	14.050624	-0.058000	4.815473
282.641518	8000.137785	14.055629	-0.057971	4.815465
282.693281	8000.130098	14.060634	-0.057981	4.815462
282.984610	8000.149876	14.065639	-0.058035	4.815467
282.673109	8000.119093	14.070643	-0.057977	4.815459
282.771667	8000.154924	14.075648	-0.057995	4.815469
282.837621	8000.149609	14.080653	-0.058008	4.815467
282.878471	8000.153497	14.085658	-0.058015	4.815468
282.749364	8000.182363	14.090663	-0.057992	4.815477
282.603513	8000.152178	14.095667	-0.057964	4.815469
282.663663	8000.180963	14.100672	-0.057976	4.815477
282.887164	8000.148327	14.105677	-0.058017	4.815467
282.835708	8000.132524	14.110682	-0.058008	4.815462
282.921025	8000.118979	14.115687	-0.058024	4.815458
282.529396	8000.107177	14.120691	-0.057951	4.815456
282.665782	8000.151113	14.125696	-0.057977	4.815468
282.929751	8000.121282	14.130701	-0.058026	4.815459
283.096398	8000.164650	14.135706	-0.058057	4.815470
282.849281	8000.226834	14.140711	-0.058011	4.815490
282.695968	8000.135612	14.145715	-0.057982	4.815464
282.780855	8000.155188	14.150720	-0.057998	4.815469
282.858542	8000.143654	14.155725	-0.058013	4.815465
282.864378	8000.128797	14.160730	-0.058014	4.815461
283.086517	8000.163463	14.165735	-0.058056	4.815470
282.977892	8000.163814	14.170739	-0.058035	4.815471
282.872092	8000.202684	14.175744	-0.058016	4.815483
283.024900	8000.247961	14.180749	-0.058044	4.815495
283.079459	8000.205054	14.185754	-0.058055	4.815482
282.862472	8000.206822	14.190759	-0.058014	4.815484
282.860382	8000.203589	14.195763	-0.058014	4.815483
282.823098	8000.202980	14.200768	-0.058007	4.815483
282.723481	8000.122263	14.205773	-0.057989	4.815460
282.771079	8000.136949	14.210778	-0.057998	4.815464
282.914968	8000.185284	14.215783	-0.058024	4.815477
282.801519	8000.134260	14.220787	-0.058003	4.815463
282.781832	8000.166002	14.225792	-0.058000	4.815472
282.939367	8000.178229	14.230797	-0.058029	4.815475
282.816034	8000.181543	14.235802	-0.058006	4.815477
282.844921	7999.254464	14.240807	-0.058011	4.815206

282.726448	7995.997920	14.245811	-0.057987	4.814255
282.951955	7990.601843	14.250816	-0.058026	4.812676
282.904051	7983.927240	14.255821	-0.058013	4.810725
282.699348	7976.639261	14.260826	-0.057970	4.808594
282.582593	7969.007189	14.265831	-0.057943	4.806362
282.592990	7961.206918	14.270835	-0.057940	4.804078
282.561837	7953.376687	14.275840	-0.057929	4.801784
282.413601	7945.322643	14.280845	-0.057896	4.799425
282.460195	7937.435228	14.285850	-0.057900	4.797112
282.473563	7929.392574	14.290855	-0.057897	4.794753
282.246451	7921.388657	14.295859	-0.057850	4.792405
282.480306	7913.352880	14.300864	-0.057888	4.790044
282.374544	7905.446839	14.305869	-0.057864	4.787722
282.151703	7897.352954	14.310874	-0.057817	4.785344
282.282460	7889.416671	14.315879	-0.057836	4.783010
282.025974	7881.354819	14.320883	-0.057783	4.780639
282.092887	7873.410635	14.325888	-0.057791	4.778300
282.188475	7865.439968	14.330893	-0.057803	4.775952
282.083570	7857.363585	14.335898	-0.057779	4.773573
281.938240	7849.384989	14.340903	-0.057746	4.771222
281.943928	7841.350924	14.345907	-0.057742	4.768852
281.894033	7833.396322	14.350912	-0.057728	4.766505
281.779698	7825.349725	14.355917	-0.057702	4.764130
281.563958	7817.405296	14.360922	-0.057656	4.761784
281.534818	7809.388937	14.365927	-0.057646	4.759415
281.680604	7801.402913	14.370931	-0.057668	4.757053
281.577183	7793.329314	14.375936	-0.057643	4.754665
281.555217	7785.321905	14.380941	-0.057634	4.752295
281.568337	7777.319951	14.385946	-0.057631	4.749925
281.451707	7769.322683	14.390951	-0.057605	4.747557
281.465490	7761.296111	14.395955	-0.057602	4.745177
281.403729	7753.348549	14.400960	-0.057585	4.742820
281.269567	7745.352676	14.405965	-0.057555	4.740448
281.274095	7737.358067	14.410970	-0.057551	4.738075
281.274263	7729.344308	14.415975	-0.057546	4.735695
281.157408	7721.298784	14.420979	-0.057519	4.733304
281.059137	7713.273302	14.425984	-0.057495	4.730918
281.146557	7705.338645	14.430989	-0.057507	4.728558
281.031459	7697.300145	14.435994	-0.057480	4.726166
281.138390	7689.322267	14.440999	-0.057495	4.723790
280.758959	7681.311619	14.446003	-0.057419	4.721404
280.798904	7673.377888	14.451008	-0.057421	4.719040
280.833924	7665.398895	14.456013	-0.057423	4.716660
280.524082	7657.296611	14.461018	-0.057360	4.714243
280.660303	7649.296281	14.466023	-0.057380	4.711855
280.645569	7641.228769	14.471027	-0.057372	4.709445
280.553856	7633.313128	14.476032	-0.057350	4.707080
280.534212	7625.293474	14.481037	-0.057341	4.704682
280.676584	7617.302052	14.486042	-0.057363	4.702291
280.582953	7609.305686	14.491047	-0.057340	4.699898
280.415131	7601.316055	14.496051	-0.057304	4.697506
280.433732	7593.252631	14.501056	-0.057302	4.695090
280.464362	7585.307975	14.506061	-0.057303	4.692709
280.281804	7577.261939	14.511066	-0.057264	4.690296
280.280229	7569.304437	14.516071	-0.057258	4.687908
280.120441	7561.257537	14.521075	-0.057223	4.685493
280.054364	7553.307872	14.526080	-0.057206	4.683105
280.188391	7545.290692	14.531085	-0.057226	4.680696
280.197914	7537.268634	14.536090	-0.057222	4.678284
280.197748	7529.282831	14.541095	-0.057217	4.675881
279.898045	7521.217748	14.546099	-0.057156	4.673454
279.903461	7513.149090	14.551104	-0.057152	4.671024
280.135762	7505.213079	14.556109	-0.057190	4.668633
279.873251	7497.203329	14.561114	-0.057136	4.666219
279.832095	7489.237038	14.566119	-0.057123	4.663816
279.779339	7481.231390	14.571123	-0.057108	4.661400
279.851970	7473.247965	14.576128	-0.057117	4.658990
279.708452	7465.230687	14.581133	-0.057085	4.656568
279.519903	7457.189611	14.586138	-0.057045	4.654138
279.681058	7449.213787	14.591143	-0.057070	4.651726
279.593134	7441.158778	14.596147	-0.057048	4.649289
279.250680	7433.219712	14.601152	-0.056979	4.646886
279.282506	7425.187962	14.606157	-0.056980	4.644453
279.157448	7417.263038	14.611162	-0.056952	4.642052
279.261089	7409.199682	14.616167	-0.056966	4.639607
279.140896	7401.239899	14.621171	-0.056938	4.637192
279.014314	7393.196895	14.626176	-0.056909	4.634751
278.955482	7385.198379	14.631181	-0.056893	4.632322
279.144335	7377.153079	14.636186	-0.056923	4.629878
278.976793	7369.225491	14.641191	-0.056887	4.627468
278.834545	7361.152310	14.646195	-0.056855	4.625012
278.948048	7353.212925	14.651200	-0.056872	4.622596
278.873633	7345.160672	14.656205	-0.056852	4.620144
278.751179	7337.225409	14.661210	-0.056825	4.617727
278.802078	7329.208385	14.666215	-0.056829	4.615283
278.593018	7321.121890	14.671219	-0.056785	4.612817
278.599233	7313.109338	14.676224	-0.056781	4.610373
278.485739	7305.181849	14.681229	-0.056755	4.607952
278.461603	7297.098104	14.686234	-0.056745	4.605483
278.460280	7289.188227	14.691239	-0.056740	4.603066
278.352766	7281.153997	14.696243	-0.056714	4.600609
278.217105	7273.204735	14.701248	-0.056684	4.598177
278.373386	7265.176770	14.706253	-0.056708	4.595720
278.207213	7257.075056	14.711258	-0.056672	4.593238
278.284234	7249.109794	14.716263	-0.056681	4.590798
278.174426	7241.109395	14.721267	-0.056656	4.588345
278.127251	7233.088777	14.726272	-0.056642	4.585884
278.177945	7225.145486	14.731277	-0.056646	4.583446
278.319571	7217.112681	14.736282	-0.056667	4.580980
278.396499	7209.151371	14.741287	-0.056676	4.578533
278.124451	7201.112034	14.746291	-0.056621	4.576062
277.973718	7193.127522	14.751296	-0.056587	4.573606
277.716422	7185.132498	14.756301	-0.056534	4.571145
277.636593	7177.114925	14.761306	-0.056514	4.568676
277.591354	7169.124901	14.766311	-0.056501	4.566214
277.576137	7161.112772	14.771315	-0.056493	4.563745
277.856638	7153.170599	14.776320	-0.056540	4.561295
277.637055	7145.141640	14.781325	-0.056494	4.558817
277.407327	7137.091914	14.786330	-0.056446	4.556332
277.537735	7129.105644	14.791335	-0.056465	4.553865
277.381332	7121.064446	14.796339	-0.056431	4.551379
277.198382	7113.100505	14.801344	-0.056392	4.548916
277.397993	7105.095607	14.806349	-0.056424	4.546439
277.344610	7097.082245	14.811354	-0.056409	4.543958
277.511930	7089.148636	14.816359	-0.056435	4.541501
277.220080	7081.093007	14.821363	-0.056375	4.539003
277.168373	7073.147191	14.826368	-0.056361	4.536539
277.057005	7065.098454	14.831373	-0.056335	4.534041
277.002489	7057.071941	14.836378	-0.056319	4.531549
277.128869	7049.098931	14.841383	-0.056338	4.529073
277.085214	7041.105274	14.846387	-0.056325	4.526589
276.849876	7033.049105	14.851392	-0.056276	4.524083
276.846688	7025.133277	14.856397	-0.056270	4.521620
276.870976	7017.114296	14.861402	-0.056269	4.519124
276.865407	7009.175119	14.866407	-0.056263	4.516651
276.759062	7001.053801	14.871411	-0.056238	4.514119
276.767255	6992.970217	14.876416	-0.056234	4.511599
276.593467	6985.030673	14.881421	-0.056197	4.509121
276.445034	6977.040370	14.886426	-0.056164	4.506626
276.364401	6969.042992	14.891431	-0.056144	4.504128
276.533477	6961.071897	14.896435	-0.056170	4.501637
276.447977	6953.035545	14.901440	-0.056149	4.499124
276.360614	6945.104495	14.906445	-0.056128	4.496642
276.275646	6937.028293	14.911450	-0.056107	4.494114
276.398312	6929.053367	14.916455	-0.056125	4.491616
276.093903	6921.053087	14.921459	-0.056063	4.489108
276.306144	6913.047356	14.926464	-0.056097	4.486598
276.211659	6905.077950	14.931469	-0.056075	4.484098
275.936629	6897.096981	14.936474	-0.056018	4.481591
275.959120	6889.059867	14.941479	-0.056017	4.479067
275.893864	6881.048075	14.946483	-0.056000	4.476549
275.783871	6872.995651	14.951488	-0.055974	4.474016
276.036843	6865.022217	14.956493	-0.056016	4.471508
276.056121	6857.034957	14.961498	-0.056015	4.468994
275.901838	6849.054166	14.966503	-0.055981	4.466479
275.552648	6841.003941	14.971507	-0.055911	4.463941
275.876240	6833.010902	14.976512	-0.055966	4.461421
275.780704	6825.042105	14.981517	-0.055943	4.458906
275.471353	6817.009269	14.986522	-0.055880	4.456369
275.505487	6809.058905	14.991527	-0.055882	4.453858
275.581752	6800.965359	14.996531	-0.055891	4.451300
275.504656	6792.997809	15.001536	-0.055871	4.448780
275.313548	6785.029382	15.006541	-0.055830	4.446258
275.285759	6776.986527	15.011546	-0.055820	4.443711
275.516202	6769.042401	15.016551	-0.055858	4.441195
275.227191	6760.991549	15.021555	-0.055799	4.438642
275.338048	6753.014765	15.026560	-0.055814	4.436113
275.173349	6745.001080	15.031565	-0.055779	4.433569
274.930246	6736.925350	15.036570	-0.055728	4.431004
275.109171	6728.977065	15.041575	-0.055756	4.428479
275.089525	6720.928124	15.046579	-0.055748	4.425920
274.964298	6712.961940	15.051584	-0.055719	4.423386
274.763071	6704.987778	15.056589	-0.055677	4.420847
274.912212	6696.956163	15.061594	-0.055699	4.418290
274.861278	6688.984114	15.066599	-0.055685	4.415750
274.648391	6680.973169	15.071603	-0.055640	4.413195
274.699070	6672.936418	15.076608	-0.055644	4.410631
274.677939	6664.952400	15.081613	-0.055635	4.408083
274.518588	6656.907799	15.086618	-0.055600	4.405513
274.467594	6648.990246	15.091623	-0.055586	4.402982
274.308233	6640.978510	15.096627	-0.055551	4.400420
274.515524	6633.017128	15.101632	-0.055584	4.397874
274.337427	6625.014106	15.106637	-0.055546	4.395311
274.178476	6616.959965	15.111642	-0.055511	4.392730
274.245014	6608.928177	15.116647	-0.055519	4.390156
274.183684	6600.954885	15.121651	-0.055502	4.387599
274.254303	6592.954775	15.126656	-0.055510	4.385033
274.173624	6584.962989	15.131661	-0.055490	4.382466
273.966858	6576.924753	15.136666	-0.055446	4.379883
274.053636	6569.016132	15.141671	-0.055457	4.377341
273.824699	6560.972309	15.146675	-0.055410	4.374753
273.815438	6552.972914	15.151680	-0.055403	4.372178
273.778842	6544.953555	15.156685	-0.055391	4.369596
273.673990	6536.981904	15.161690	-0.055366	4.367027
273.824835	6528.980092	15.166695	-0.055389	4.364448
273.498602	6520.995076	15.171699	-0.055323	4.361870
273.395721	6512.976717	15.176704	-0.055299	4.359281
273.483614	6505.003865	15.181709	-0.055310	4.356707
273.490459	6496.931072	15.186714	-0.055306	4.354098
273.241660	6488.888529	15.191719	-0.055255	4.351496
273.435955	6480.897864	15.196723	-0.055286	4.348912
273.196900	6472.900508	15.201728	-0.055236	4.346321
273.003163	6464.957189	15.206733	-0.055195	4.343747
273.061558	6456.909408	15.211738	-0.055201	4.341139
273.364906	6448.973882	15.216743	-0.055252	4.338567
273.075654	6440.962252	15.221747	-0.055193	4.335965
272.961944	6432.931604	15.226752	-0.055167	4.333357
273.003104	6424.927469	15.231757	-0.055169	4.330757
272.881685	6416.921123	15.236762	-0.055142	4.328153
272.808584	6408.942572	15.241767	-0.055123	4.325557
272.879186	6400.939765	15.246771	-0.055131	4.322953
272.833227	6392.938624	15.251776	-0.055117	4.320346
272.810360	6384.963842	15.256781	-0.055108	4.317747
272.792126	6376.893275	15.261786	-0.055099	4.315115
272.762396	6368.940783	15.266791	-0.055089	4.312520
272.464214	6360.890345	15.271795	-0.055028	4.309890
272.341124	6352.904864	15.276800	-0.055000	4.307280
272.527327	6344.913167	15.281805	-0.055029	4.304669
272.518892	6336.902253	15.286810	-0.055023	4.302049
272.540530	6328.906953	15.291815	-0.055022	4.299432
272.546646	6320.930238	15.296819	-0.055018	4.296820
272.342672	6312.894918	15.301824	-0.054975	4.294185
272.316468	6304.938308	15.306829	-0.054965	4.291576
272.192839	6296.874812	15.311834	-0.054936	4.288930
272.363361	6288.902183	15.316839	-0.054963	4.286314
272.189029	6280.893621	15.321843	-0.054925	4.283682
272.205128	6272.908975	15.326848	-0.054923	4.281057
272.167806	6264.932487	15.331853	-0.054911	4.278434
271.933523	6256.911922	15.336858	-0.054862	4.275792
271.909019	6248.903303	15.341863	-0.054853	4.273155
271.782197	6240.861587	15.346867	-0.054824	4.270504
271.691667	6232.899697	15.351872	-0.054802	4.267878
271.513670	6224.838170	15.356877	-0.054764	4.265217
271.703615	6216.862695	15.361882	-0.054794	4.262586
271.768796	6208.851967	15.366887	-0.054801	4.259940
271.664596	6200.911213	15.371891	-0.054776	4.257314
271.491349	6192.869713	15.376896	-0.054739	4.254653
271.515113	6184.873180	15.381901	-0.054738	4.252007
271.456371	6176.849033	15.386906	-0.054722	4.249349
271.338980	6168.934235	15.391911	-0.054695	4.246725
271.207571	6160.885465	15.396915	-0.054666	4.244055
271.202647	6152.926676	15.401920	-0.054660	4.241415
271.385142	6144.901718	15.406925	-0.054689	4.238752
270.952283	6136.923773	15.411930	-0.054603	4.236098
270.985717	6128.918798	15.416935	-0.054604	4.233438
271.015709	6120.864526	15.421939	-0.054604	4.230759
270.971636	6112.878466	15.426944	-0.054591	4.228100
270.927335	6104.859976	15.431949	-0.054578	4.225430
270.731627	6096.910999	15.436954	-0.054536	4.222779
270.799722	6088.958309	15.441959	-0.054544	4.220128
270.558552	6080.944101	15.446963	-0.054494	4.217451
270.807069	6072.925922	15.451968	-0.054535	4.214776
270.763111	6064.906673	15.456973	-0.054521	4.212097
270.616346	6056.896627	15.461978	-0.054489	4.209417
270.793464	6048.910712	15.466983	-0.054517	4.206748
270.649937	6040.888441	15.471987	-0.054485	4.204061
270.564386	6032.941308	15.476992	-0.054464	4.201398
270.573544	6024.933898	15.481997	-0.054460	4.198715
270.408730	6016.930580	15.487002	-0.054425	4.196029
270.346506	6008.830629	15.492007	-0.054408	4.193310
270.176022	6000.808195	15.497011	-0.054371	4.190614
270.040293	5992.833537	15.502016	-0.054341	4.187933
270.201960	5984.860940	15.507021	-0.054366	4.185254
269.810424	5976.895596	15.512026	-0.054288	4.182570
269.939708	5968.886063	15.517031	-0.054307	4.179874
269.889401	5960.914422	15.522035	-0.054292	4.177188
270.134107	5952.854858	15.527040	-0.054332	4.174474
270.076151	5944.860472	15.532045	-0.054317	4.171776
270.029483	5936.867212	15.537050	-0.054303	4.169078
270.004000	5928.891377	15.542055	-0.054293	4.166383
269.921384	5920.869096	15.547059	-0.054272	4.163671
269.980804	5912.887851	15.552064	-0.054278	4.160972
269.961568	5904.931060	15.557069	-0.054270	4.158279
269.614499	5896.888428	15.562074	-0.054200	4.155552
269.698723	5888.878660	15.567079	-0.054210	4.152838
269.821594	5880.837780	15.572083	-0.054228	4.150113
269.614807	5872.850470	15.577088	-0.054184	4.147400
269.532235	5864.860430	15.582093	-0.054164	4.144687
269.344201	5856.882152	15.587098	-0.054124	4.141973
269.331673	5848.872647	15.592103	-0.054116	4.139250
269.139761	5840.879432	15.597107	-0.054075	4.136528
269.210363	5832.869285	15.602112	-0.054084	4.133802
269.294202	5824.827277	15.607117	-0.054094	4.131064
269.025945	5816.850070	15.612122	-0.054039	4.128341
269.189530	5808.845986	15.617127	-0.054064	4.125613
269.255515	5800.897355	15.622131	-0.054071	4.122900
269.231264	5792.884172	15.627136	-0.054062	4.120163
269.212540	5784.930912	15.632141	-0.054053	4.117444
268.979035	5776.882352	15.637146	-0.054005	4.114688
268.884327	5768.856875	15.642151	-0.053982	4.111940
268.773562	5760.808256	15.647155	-0.053956	4.109182
268.682046	5752.836305	15.652160	-0.053934	4.106449
268.697142	5744.853813	15.657165	-0.053932	4.103712
268.393893	5736.888842	15.662170	-0.053870	4.100974
268.498262	5728.901814	15.667175	-0.053884	4.098233
268.406742	5720.871366	15.672179	-0.053862	4.095472
268.323258	5712.872385	15.677184	-0.053841	4.092720
268.350461	5704.859081	15.682189	-0.053841	4.089963
268.351481	5696.871239	15.687194	-0.053836	4.087213
268.410911	5688.879229	15.692199	-0.053842	4.084460
268.059916	5680.947788	15.697203	-0.053772	4.081720
268.108258	5672.912743	15.702208	-0.053776	4.078949
268.081525	5664.957563	15.707213	-0.053766	4.076202
267.898325	5656.900244	15.712218	-0.053726	4.073415
267.981638	5648.873853	15.717223	-0.053737	4.070641
268.015828	5640.870236	15.722227	-0.053738	4.067873
267.900014	5632.871874	15.727232	-0.053711	4.065102
268.031904	5624.911200	15.732237	-0.053731	4.062346
267.921982	5616.891128	15.737242	-0.053705	4.059564
267.923635	5608.939457	15.742247	-0.053700	4.056805
267.529753	5600.910764	15.747251	-0.053622	4.054012
267.586883	5592.894981	15.752256	-0.053627	4.051228
267.542833	5584.932031	15.757261	-0.053614	4.048460
267.345435	5576.867087	15.762266	-0.053572	4.045651
267.325300	5568.927624	15.767271	-0.053563	4.042887
267.500868	5560.920774	15.772275	-0.053591	4.040100
267.345643	5552.939793	15.777280	-0.053557	4.037316
267.272384	5544.908980	15.782285	-0.053538	4.034513
267.248143	5536.765449	15.787290	-0.053528	4.031670
267.327711	5528.835806	15.792295	-0.053538	4.028901
267.094675	5520.877879	15.797299	-0.053490	4.026115
267.039261	5512.875866	15.802304	-0.053474	4.023315
267.212873	5504.911298	15.807309	-0.053501	4.020530
266.934813	5496.905289	15.812314	-0.053444	4.017721
266.829269	5488.892018	15.817319	-0.053420	4.014910
266.875414	5480.848301	15.822323	-0.053423	4.012089
266.839274	5472.848579	15.827328	-0.053411	4.009280
266.748814	5464.896901	15.832333	-0.053389	4.006485
266.794586	5456.907389	15.837338	-0.053393	4.003678
266.689364	5448.914336	15.842343	-0.053368	4.000864
266.557446	5440.936150	15.847347	-0.053338	3.998053
266.507939	5432.900519	15.852352	-0.053324	3.995222
266.662271	5424.890479	15.857357	-0.053347	3.992400
266.372320	5416.831309	15.862362	-0.053288	3.989552
266.447531	5408.896388	15.867367	-0.053297	3.986752
266.561326	5400.866288	15.872371	-0.053313	3.983917
266.508166	5392.893784	15.877376	-0.053298	3.981098
266.539486	5384.916828	15.882381	-0.053299	3.978276
266.317004	5376.915146	15.887386	-0.053252	3.975439
266.511698	5368.907509	15.892391	-0.053284	3.972605
266.095558	5360.898376	15.897395	-0.053201	3.969759
265.856346	5352.938645	15.902400	-0.053151	3.966931
266.095970	5344.901167	15.907405	-0.053191	3.964081
266.057443	5336.939812	15.912410	-0.053178	3.961251
265.912929	5328.952411	15.917415	-0.053146	3.958409
265.798394	5320.940423	15.922419	-0.053120	3.955556
265.710515	5312.925087	15.927424	-0.053098	3.952700
265.738151	5304.930099	15.932429	-0.053098	3.949852
265.748915	5296.912820	15.937434	-0.053095	3.946993
265.916582	5288.925123	15.942439	-0.053121	3.944145
265.640533	5280.965896	15.947443	-0.053065	3.941298
265.657353	5272.962235	15.952448	-0.053063	3.938438
265.682769	5264.957852	15.957453	-0.053063	3.935576
265.525994	5256.925655	15.962458	-0.053028	3.932698
265.492382	5248.929835	15.967463	-0.053017	3.929834
265.382402	5240.978536	15.972467	-0.052991	3.926982
265.282911	5232.935089	15.977472	-0.052968	3.924095
265.270897	5224.980988	15.982477	-0.052960	3.921239
264.969680	5216.951842	15.987482	-0.052899	3.918350
265.101979	5208.986479	15.992487	-0.052918	3.915489
265.126391	5200.984707	15.997491	-0.052918	3.912611
264.737982	5192.926848	16.002496	-0.052840	3.909702
264.962982	5184.950877	16.007501	-0.052877	3.906833
264.925886	5176.962242	16.012506	-0.052865	3.903952
264.979012	5168.982614	16.017511	-0.052870	3.901074
264.690515	5160.964478	16.022515	-0.052811	3.898173
264.700988	5152.947990	16.027520	-0.052808	3.895277
264.777019	5144.951277	16.032525	-0.052817	3.892386
264.587904	5136.937402	16.037530	-0.052777	3.889482
264.705371	5128.980560	16.042535	-0.052793	3.886603
264.683461	5120.964656	16.047539	-0.052784	3.883697
264.573141	5112.953466	16.052544	-0.052758	3.880790
264.611000	5105.016912	16.057549	-0.052760	3.877909
264.472733	5096.973721	16.062554	-0.052730	3.874985
264.456092	5088.747245	16.067559	-0.052721	3.871994
264.315262	5080.822954	16.072563	-0.052690	3.869109
264.292179	5072.820235	16.077568	-0.052680	3.866194
264.271227	5064.904820	16.082573	-0.052671	3.863310
263.855449	5056.919382	16.087578	-0.052589	3.860390
264.050984	5048.956180	16.092583	-0.052620	3.857488
264.137531	5040.926280	16.097587	-0.052631	3.854558
263.894533	5032.940335	16.102592	-0.052581	3.851634
263.933308	5024.973928	16.107597	-0.052583	3.848721
263.901994	5016.927920	16.112602	-0.052572	3.845776
263.890937	5009.007094	16.117607	-0.052565	3.842874
263.695185	5000.980884	16.122611	-0.052523	3.839928
263.807138	4993.027816	16.127616	-0.052539	3.837013
263.769892	4985.022027	16.132621	-0.052527	3.834073
263.591962	4976.948838	16.137626	-0.052489	3.831103
263.641776	4968.994647	16.142631	-0.052493	3.828179
263.703258	4960.978006	16.147635	-0.052499	3.825230
263.367932	4953.023302	16.152640	-0.052431	3.822294
263.470644	4945.023440	16.157645	-0.052445	3.819347
263.316070	4937.028472	16.162650	-0.052412	3.816395
263.437517	4929.057612	16.167655	-0.052429	3.813455
263.202546	4921.016392	16.172659	-0.052380	3.810480
263.325091	4913.038397	16.177664	-0.052398	3.807533
263.388004	4905.032061	16.182669	-0.052404	3.804572
263.239499	4897.084787	16.187674	-0.052372	3.801626
263.090497	4889.084822	16.192679	-0.052339	3.798658
263.067764	4881.087093	16.197683	-0.052329	3.795692
262.884842	4873.032807	16.202688	-0.052290	3.792698
262.839701	4865.022149	16.207693	-0.052277	3.789722
262.759521	4857.037528	16.212698	-0.052257	3.786752
262.705177	4849.051797	16.217703	-0.052241	3.783780
262.708325	4841.047128	16.222707	-0.052237	3.780800
262.435146	4833.068754	16.227712	-0.052181	3.777821
262.624514	4825.033726	16.232717	-0.052211	3.774828
262.390328	4817.067438	16.237722	-0.052162	3.771850
262.529332	4809.035580	16.242727	-0.052183	3.768853
262.296662	4801.100334	16.247731	-0.052135	3.765882
262.143633	4793.075661	16.252736	-0.052101	3.762876
262.098268	4785.106715	16.257741	-0.052087	3.759892
262.169192	4777.109482	16.262746	-0.052095	3.756897
262.232629	4769.058313	16.267751	-0.052102	3.753879
262.203673	4761.056737	16.272755	-0.052092	3.750875
262.025455	4753.043443	16.277760	-0.052053	3.747861
262.055920	4745.070996	16.282765	-0.052054	3.744865
261.895571	4737.101917	16.287770	-0.052019	3.741863
261.862172	4729.097367	16.292775	-0.052008	3.738849
262.044646	4721.070811	16.297779	-0.052036	3.735828
261.890541	4713.069422	16.302784	-0.052003	3.732807
261.748912	4705.088677	16.307789	-0.051971	3.729792
261.770539	4697.118965	16.312794	-0.051970	3.726782
261.799631	4689.119715	16.317799	-0.051970	3.723758
261.539826	4681.152827	16.322803	-0.051917	3.720738
261.594980	4673.162466	16.327808	-0.051922	3.717714
261.654618	4665.163477	16.332813	-0.051928	3.714684
261.268911	4657.067221	16.337818	-0.051851	3.711604
261.278816	4649.063278	16.342823	-0.051848	3.708565
261.363481	4641.107051	16.347827	-0.051858	3.705545
261.274257	4633.139037	16.352832	-0.051837	3.702513
261.187337	4625.126599	16.357837	-0.051815	3.699462
261.247916	4617.143125	16.362842	-0.051821	3.696423
261.385443	4609.136587	16.367847	-0.051842	3.693375
261.111359	4601.154685	16.372851	-0.051786	3.690323
261.123518	4593.172886	16.377856	-0.051783	3.687276
261.034586	4585.188858	16.382861	-0.051761	3.684223
260.978175	4577.194646	16.387866	-0.051746	3.681164
260.892419	4569.216400	16.392871	-0.051724	3.678108
260.997986	4561.216579	16.397875	-0.051739	3.675047
260.785057	4553.157610	16.402880	-0.051694	3.671952
260.884820	4545.191896	16.407885	-0.051708	3.668898
260.529675	4537.188648	16.412890	-0.051636	3.665815
260.611415	4529.214756	16.417895	-0.051646	3.662752
260.482816	4521.209017	16.422899	-0.051617	3.659669
260.271162	4513.242476	16.427904	-0.051573	3.656597
260.408350	4505.220097	16.432909	-0.051593	3.653509
260.365170	4497.158503	16.437914	-0.051580	3.650399
260.319936	4489.196923	16.442919	-0.051567	3.647325
260.268326	4481.208591	16.447923	-0.051552	3.644237
260.265106	4473.256816	16.452928	-0.051546	3.641163
260.282632	4465.261138	16.457933	-0.051544	3.638069
260.179266	4457.224231	16.462938	-0.051520	3.634954
260.133386	4449.215230	16.467943	-0.051506	3.631848
260.107197	4441.209321	16.472947	-0.051496	3.628741
260.036936	4433.212560	16.477952	-0.051478	3.625634
260.155260	4425.265691	16.482957	-0.051495	3.622549
259.955970	4417.217079	16.487962	-0.051453	3.619413
259.789390	4409.314315	16.492967	-0.051417	3.616332
259.799518	4401.239296	16.497971	-0.051413	3.613186
259.734233	4393.205460	16.502976	-0.051396	3.610051
259.495374	4385.302096	16.507981	-0.051346	3.606960
259.435131	4377.265088	16.512986	-0.051330	3.603818
259.629735	4369.298334	16.517991	-0.051361	3.600709
259.538518	4361.338109	16.522995	-0.051339	3.597591
259.290105	4353.327596	16.528000	-0.051288	3.594447
259.374143	4345.318589	16.533005	-0.051298	3.591309
259.281856	4337.297460	16.538010	-0.051276	3.588160
259.259263	4329.326852	16.543015	-0.051267	3.585029
259.278331	4321.369726	16.548019	-0.051265	3.581902
259.046755	4313.368768	16.553024	-0.051217	3.578748
259.127059	4305.386302	16.558029	-0.051227	3.575607
258.968100	4297.342007	16.563034	-0.051192	3.572432
258.837176	4289.356683	16.568039	-0.051162	3.569279
258.858710	4281.375965	16.573043	-0.051161	3.566128
258.866300	4273.359886	16.578048	-0.051157	3.562961
258.837652	4265.412794	16.583053	-0.051147	3.559817
258.683037	4257.407184	16.588058	-0.051113	3.556644
258.582145	4249.366997	16.593063	-0.051089	3.553455
258.631066	4241.293800	16.598067	-0.051093	3.550255
258.579554	4233.314775	16.603072	-0.051078	3.547087
258.534961	4225.357314	16.608077	-0.051065	3.543924
258.593382	4217.346666	16.613082	-0.051071	3.540741
258.490231	4209.405545	16.618087	-0.051046	3.537577
258.581961	4201.399685	16.623091	-0.051058	3.534391
258.385316	4193.381344	16.628096	-0.051017	3.531188
258.401950	4185.401114	16.633101	-0.051015	3.528004
258.395749	4177.372790	16.638106	-0.051008	3.524797
258.266611	4169.461063	16.643111	-0.050979	3.521630
258.220120	4161.462077	16.648115	-0.050965	3.518428
257.964810	4153.468481	16.653120	-0.050913	3.515218
258.048679	4145.447690	16.658125	-0.050923	3.512005
257.923055	4137.437895	16.663130	-0.050895	3.508788
257.830068	4129.444645	16.668135	-0.050872	3.505574
257.751695	4121.482482	16.673139	-0.050853	3.502371
257.633173	4113.494307	16.678144	-0.050825	3.499153
258.014583	4105.524243	16.683149	-0.050891	3.495956
257.821264	4097.483805	16.688154	-0.050850	3.492708
257.574371	4089.503078	16.693159	-0.050799	3.489481
257.726359	4081.526412	16.698163	-0.050822	3.486264
257.602977	4073.526953	16.703168	-0.050794	3.483026
257.491848	4065.567193	16.708173	-0.050768	3.479802
257.306629	4057.592975	16.713178	-0.050729	3.476567
257.407162	4049.512049	16.718183	-0.050742	3.473294
257.362575	4041.507892	16.723187	-0.050729	3.470045
257.236208	4033.515455	16.728192	-0.050700	3.466795
257.103967	4025.554841	16.733197	-0.050670	3.463555
257.091195	4017.555384	16.738202	-0.050663	3.460300
257.190767	4009.576685	16.743207	-0.050676	3.457054
257.047429	4001.582844	16.748211	-0.050645	3.453790
256.917547	3993.561898	16.753216	-0.050615	3.450513
257.160677	3985.585774	16.758221	-0.050655	3.447263
256.877470	3977.583302	16.763226	-0.050598	3.443982
256.775108	3969.611297	16.768231	-0.050573	3.440717
256.845778	3961.619138	16.773235	-0.050581	3.437445
256.775617	3953.616347	16.778240	-0.050563	3.434162
256.583055	3945.636565	16.783245	-0.050522	3.430881
256.523290	3937.627813	16.788250	-0.050506	3.427589
256.537078	3929.622272	16.793255	-0.050503	3.424298
256.494072	3921.682927	16.798259	-0.050490	3.421029
256.592832	3913.659219	16.803264	-0.050504	3.417727
256.509412	3905.687032	16.808269	-0.050483	3.414436
256.164535	3897.661821	16.813274	-0.050414	3.411112
256.257949	3889.683744	16.818279	-0.050426	3.407819
256.330299	3881.668311	16.823283	-0.050434	3.404506
256.253416	3873.722092	16.828288	-0.050415	3.401214
256.105539	3865.767702	16.833293	-0.050382	3.397913
255.948500	3857.736119	16.838298	-0.050348	3.394576
255.974200	3849.643053	16.843303	-0.050347	3.391217
255.949002	3841.668150	16.848307	-0.050337	3.387902
255.737497	3833.689032	16.853312	-0.050293	3.384575
255.740261	3825.771684	16.858317	-0.050288	3.381278
255.752173	3817.740758	16.863322	-0.050285	3.377931
255.648373	3809.782962	16.868327	-0.050261	3.374607
255.568414	3801.772753	16.873331	-0.050241	3.371259
255.528375	3793.741761	16.878336	-0.050228	3.367900
255.629604	3785.783525	16.883341	-0.050242	3.364573
255.537497	3777.845963	16.888346	-0.050220	3.361245
255.384508	3769.832241	16.893351	-0.050186	3.357879
255.260623	3761.849402	16.898355	-0.050158	3.354524
255.255174	3753.808691	16.903360	-0.050152	3.351145
255.153715	3745.840786	16.908365	-0.050128	3.347790
254.880872	3737.818695	16.913370	-0.050072	3.344403
254.793002	3729.875423	16.918375	-0.050051	3.341052
254.900429	3721.875824	16.923379	-0.050065	3.337681
254.915291	3713.870169	16.928384	-0.050063	3.334301
254.915709	3705.867249	16.933389	-0.050058	3.330918
254.837796	3697.878591	16.938394	-0.050038	3.327534
254.770042	3689.876580	16.943399	-0.050021	3.324142
254.699630	3681.945560	16.948403	-0.050002	3.320777
254.594673	3673.936710	16.953408	-0.049978	3.317374
254.789983	3665.940429	16.958413	-0.050009	3.313983
254.531482	3657.900015	16.963418	-0.049956	3.310554
254.442331	3649.933639	16.968423	-0.049934	3.307159
254.371461	3641.961417	16.973427	-0.049916	3.303758
254.366857	3633.971051	16.978432	-0.049910	3.300349
254.340629	3626.013530	16.983437	-0.049900	3.296949
254.244911	3617.999661	16.988442	-0.049877	3.293520
254.136277	3609.993162	16.993447	-0.049851	3.290089
254.026811	3602.030106	16.998451	-0.049826	3.286673
253.914836	3594.027590	17.003456	-0.049800	3.283237
254.134823	3586.031862	17.008461	-0.049836	3.279812
253.813710	3578.088294	17.013466	-0.049771	3.276386
253.853584	3570.055163	17.018471	-0.049773	3.272932
253.856625	3562.051235	17.023475	-0.049769	3.269485
253.761733	3554.063227	17.028480	-0.049746	3.266037
253.648641	3546.095487	17.033485	-0.049720	3.262594
253.579342	3538.085987	17.038490	-0.049702	3.259130
253.614240	3530.119491	17.043495	-0.049703	3.255686
253.516422	3522.121719	17.048499	-0.049680	3.252220
253.342161	3514.100690	17.053504	-0.049642	3.248736
253.640638	3506.112325	17.058509	-0.049693	3.245282
253.440643	3498.175547	17.063514	-0.049650	3.241826
253.392606	3490.191630	17.068519	-0.049636	3.238353
253.377236	3482.208254	17.073523	-0.049628	3.234877
253.129563	3474.128345	17.078528	-0.049577	3.231346
253.097119	3466.165355	17.083533	-0.049566	3.227871
253.027380	3458.139423	17.088538	-0.049548	3.224363
253.091448	3450.184673	17.093543	-0.049554	3.220888
253.215319	3442.202212	17.098547	-0.049572	3.217400
252.938638	3434.214025	17.103552	-0.049516	3.213888
253.067837	3426.206425	17.108557	-0.049535	3.210381
252.899800	3418.240551	17.113562	-0.049498	3.206876
252.701921	3410.275647	17.118567	-0.049456	3.203367
252.920292	3402.262386	17.123571	-0.049492	3.199850
252.834778	3394.334860	17.128576	-0.049471	3.196354
252.835355	3386.308809	17.133581	-0.049466	3.192814
252.472392	3378.308667	17.138586	-0.049393	3.189267
252.420272	3370.316138	17.143591	-0.049378	3.185731
252.426660	3362.343830	17.148595	-0.049374	3.182204
252.183769	3354.342299	17.153600	-0.049324	3.178649
252.192921	3346.388928	17.158605	-0.049321	3.175122
252.332715	3338.348178	17.163610	-0.049341	3.171558
252.277080	3330.357026	17.168615	-0.049326	3.168003
252.225271	3322.387827	17.173619	-0.049311	3.164455
252.149034	3314.406849	17.178624	-0.049292	3.160896
252.016870	3306.469014	17.183629	-0.049262	3.157350
252.094081	3298.434537	17.188634	-0.049271	3.153766
251.895747	3290.412290	17.193639	-0.049229	3.150172
251.974373	3282.452425	17.198643	-0.049239	3.146613
251.694264	3274.440537	17.203648	-0.049182	3.143011
251.819618	3266.476118	17.208653	-0.049200	3.139444
251.566781	3258.516861	17.213658	-0.049148	3.135859
251.487920	3250.521943	17.218663	-0.049128	3.132261
251.491039	3242.518460	17.223667	-0.049123	3.128659
251.517008	3234.528169	17.228672	-0.049123	3.125059
251.555938	3226.554780	17.233677	-0.049125	3.121464
251.235925	3218.596476	17.238682	-0.049060	3.117855
251.280738	3210.589192	17.243687	-0.049064	3.114237
251.327435	3202.582736	17.248691	-0.049067	3.110614
251.208739	3194.584197	17.253696	-0.049040	3.106984
251.192827	3186.613669	17.258701	-0.049032	3.103366
251.204887	3178.622857	17.263706	-0.049029	3.099737
251.165692	3170.657522	17.268711	-0.049017	3.096112
251.091133	3162.653705	17.273715	-0.048998	3.092464
250.911141	3154.667945	17.278720	-0.048959	3.088815
250.815423	3146.698927	17.283725	-0.048936	3.085173
250.777253	3138.732865	17.288730	-0.048924	3.081531
250.649410	3130.765554	17.293735	-0.048895	3.077880
250.959678	3122.739432	17.298739	-0.048948	3.074218
250.715618	3114.667547	17.303744	-0.048897	3.070504
250.681072	3106.706505	17.308749	-0.048885	3.066847
250.543741	3098.747831	17.313754	-0.048855	3.063182
250.406481	3090.761464	17.318759	-0.048824	3.059500
250.169334	3082.825493	17.323763	-0.048775	3.055831
250.144882	3074.802263	17.328768	-0.048765	3.052128
250.182247	3066.819571	17.333773	-0.048767	3.048442
250.087476	3058.849347	17.338778	-0.048744	3.044752
250.063206	3050.871447	17.343783	-0.048735	3.041056
250.218276	3042.890084	17.348787	-0.048758	3.037363
250.034875	3034.890263	17.353792	-0.048719	3.033641
249.937433	3026.897469	17.358797	-0.048696	3.029921
249.819817	3018.919994	17.363802	-0.048669	3.026203
249.851481	3010.934141	17.368807	-0.048669	3.022484
249.601969	3002.975436	17.373811	-0.048618	3.018759
249.462432	2994.988455	17.378816	-0.048587	3.015022
249.484566	2986.993833	17.383821	-0.048586	3.011284
249.577046	2978.990412	17.388826	-0.048598	3.007541
249.512400	2971.006120	17.393831	-0.048581	3.003795
249.428511	2963.055788	17.398835	-0.048560	3.000058
249.190025	2955.090574	17.403840	-0.048511	2.996303
249.197283	2947.086927	17.408845	-0.048507	2.992537
249.064163	2939.070489	17.413850	-0.048477	2.988753
249.097248	2931.075723	17.418855	-0.048478	2.984983
249.037888	2923.130598	17.423859	-0.048462	2.981227
249.006042	2915.139154	17.428864	-0.048451	2.977445
249.135774	2907.151169	17.433869	-0.048470	2.973669
248.902161	2899.141069	17.438874	-0.048421	2.969859
248.756841	2891.196965	17.443879	-0.048389	2.966080
248.786110	2883.222007	17.448883	-0.048389	2.962290
248.789012	2875.227959	17.453888	-0.048385	2.958485
248.820998	2867.262663	17.458893	-0.048385	2.954690
248.530682	2859.255422	17.463898	-0.048326	2.950854
248.519980	2851.263118	17.468903	-0.048319	2.947034
248.603580	2843.282053	17.473907	-0.048330	2.943220
248.421683	2835.301680	17.478912	-0.048291	2.939387
248.513349	2827.358656	17.483917	-0.048303	2.935581
248.293818	2819.359748	17.488922	-0.048257	2.931727
248.104202	2811.376645	17.493927	-0.048216	2.927877
248.250845	2803.392659	17.498931	-0.048238	2.924040
248.238416	2795.407379	17.503936	-0.048231	2.920188
248.358939	2787.445843	17.508941	-0.048248	2.916350
248.099546	2779.406125	17.513946	-0.048195	2.912449
248.018045	2771.402202	17.518951	-0.048175	2.908569
248.028874	2763.441295	17.523955	-0.048171	2.904710
247.826072	2755.475354	17.528960	-0.048129	2.900832
247.923221	2747.500466	17.533965	-0.048142	2.896960
247.828493	2739.510666	17.538970	-0.048119	2.893066
247.623048	2731.543967	17.543975	-0.048075	2.889171
247.600932	2723.556865	17.548979	-0.048066	2.885272
247.519852	2715.605015	17.553984	-0.048046	2.881381
247.467394	2707.633983	17.558989	-0.048031	2.877477
247.280001	2699.637317	17.563994	-0.047991	2.873547
247.379757	2691.598555	17.568999	-0.048004	2.869608
247.486260	2683.653187	17.574003	-0.048019	2.865709
247.240039	2675.697347	17.579008	-0.047968	2.861780
247.342028	2667.724133	17.584013	-0.047982	2.857857
247.382761	2659.714980	17.589018	-0.047985	2.853907
247.228989	2651.715501	17.594023	-0.047951	2.849945
247.318506	2643.765272	17.599027	-0.047962	2.846016
247.129572	2635.797089	17.604032	-0.047922	2.842057
247.100185	2627.844003	17.609037	-0.047912	2.838109
247.099570	2619.859174	17.614042	-0.047906	2.834142
247.035498	2611.823162	17.619047	-0.047889	2.830139
246.931433	2603.881375	17.624051	-0.047865	2.826176
246.588498	2595.907441	17.629056	-0.047796	2.822177
246.584227	2587.941806	17.634061	-0.047790	2.818196
246.558335	2579.955619	17.639066	-0.047780	2.814198
246.460545	2571.949835	17.644071	-0.047757	2.810180
246.391618	2563.991395	17.649075	-0.047739	2.806182
246.485730	2555.993262	17.654080	-0.047751	2.802168
246.350656	2548.055934	17.659085	-0.047721	2.798165
246.205075	2540.074306	17.664090	-0.047689	2.794134
246.164999	2532.053736	17.669095	-0.047676	2.790083
246.285950	2524.097124	17.674099	-0.047693	2.786068
246.198759	2516.109547	17.679104	-0.047672	2.782020
246.267513	2508.156104	17.684109	-0.047680	2.777992
246.243986	2500.167772	17.689114	-0.047670	2.773935
246.142736	2492.170152	17.694119	-0.047646	2.769862
246.180851	2484.212768	17.699123	-0.047648	2.765813
246.052810	2476.257122	17.704128	-0.047619	2.761748
245.919525	2468.310208	17.709133	-0.047589	2.757682
245.773695	2460.302148	17.714138	-0.047557	2.753577
245.530606	2452.252396	17.719143	-0.047507	2.749439
245.535522	2444.289022	17.724147	-0.047503	2.745355
245.284674	2436.337963	17.729152	-0.047451	2.741254
245.368346	2428.366017	17.734157	-0.047461	2.737158
245.407815	2420.373663	17.739162	-0.047463	2.733042
245.363045	2412.391841	17.744167	-0.047450	2.728920
245.396168	2404.423703	17.749171	-0.047451	2.724803
245.222756	2396.474108	17.754176	-0.047414	2.720678
245.390425	2388.515830	17.759181	-0.047440	2.716562
245.160632	2380.537103	17.764186	-0.047392	2.712405
245.063536	2372.535055	17.769191	-0.047369	2.708238
245.227094	2364.553659	17.774195	-0.047394	2.704091
244.987510	2356.602919	17.779200	-0.047344	2.699929
244.801482	2348.672463	17.784205	-0.047305	2.695774
244.816380	2340.656797	17.789210	-0.047302	2.691581
244.863366	2332.672360	17.794215	-0.047306	2.687400
244.557470	2324.752477	17.799219	-0.047244	2.683224
244.559465	2316.755606	17.804224	-0.047239	2.679020
244.513861	2308.817343	17.809229	-0.047225	2.674837
244.344209	2300.804246	17.814234	-0.047189	2.670601
244.422339	2292.813982	17.819239	-0.047198	2.666385
244.328461	2284.843108	17.824243	-0.047176	2.662163
244.272199	2276.873866	17.829248	-0.047160	2.657936
244.282316	2268.899225	17.834253	-0.047157	2.653705
244.357702	2260.892040	17.839258	-0.047166	2.649453
244.159584	2252.950231	17.844263	-0.047124	2.645212
244.200438	2244.996317	17.849267	-0.047126	2.640973
244.024942	2237.043498	17.854272	-0.047088	2.636714
244.029255	2229.057866	17.859277	-0.047084	2.632442
243.922260	2221.077384	17.864282	-0.047059	2.628158
243.769254	2213.113622	17.869287	-0.047025	2.623874
243.905605	2205.143392	17.874291	-0.047046	2.619598
243.830095	2197.179332	17.879296	-0.047027	2.615304
243.705127	2189.206482	17.884301	-0.046998	2.610995
243.598280	2181.243454	17.889306	-0.046973	2.606686
243.547155	2173.273458	17.894311	-0.046959	2.602369
243.523589	2165.326511	17.899315	-0.046949	2.598060
243.344883	2157.295228	17.904320	-0.046911	2.593687
243.376207	2149.174754	17.909325	-0.046911	2.589272
243.195229	2141.246141	17.914330	-0.046872	2.584940
243.124211	2133.323696	17.919335	-0.046854	2.580611
243.187849	2125.379399	17.924339	-0.046861	2.576273
242.930341	2117.422214	17.929344	-0.046808	2.571898
242.937026	2109.447688	17.934349	-0.046804	2.567524
242.923709	2101.491538	17.939354	-0.046796	2.563152
242.866341	2093.546320	17.944359	-0.046781	2.558775
242.954777	2085.583249	17.949363	-0.046792	2.554390
242.625473	2077.614764	17.954368	-0.046726	2.549966
242.745529	2069.636767	17.959373	-0.046743	2.545561
242.742568	2061.671269	17.964378	-0.046737	2.541146
242.509190	2053.736044	17.969383	-0.046689	2.536724
242.582451	2045.759680	17.974387	-0.046697	2.532293
242.259547	2037.803904	17.979392	-0.046632	2.527838
242.296438	2029.836975	17.984397	-0.046634	2.523394
242.429422	2021.863087	17.989402	-0.046653	2.518945
242.417178	2013.885085	17.994407	-0.046646	2.514476
242.248101	2005.909468	17.999411	-0.046609	2.509989
242.157348	1997.921756	18.004416	-0.046587	2.505492
242.187233	1989.973035	18.009421	-0.046588	2.501018
242.040490	1982.023724	18.014426	-0.046555	2.496523
241.872680	1974.068081	18.019431	-0.046519	2.492015
242.151385	1966.055323	18.024435	-0.046566	2.487499
241.951840	1958.124475	18.029440	-0.046524	2.482986
241.730905	1950.204903	18.034445	-0.046477	2.478469
241.738753	1942.234517	18.039450	-0.046474	2.473933
241.644782	1934.238137	18.044455	-0.046451	2.469365
241.684001	1926.272248	18.049459	-0.046453	2.464817
241.466224	1918.333367	18.054464	-0.046408	2.460256
241.456803	1910.379348	18.059469	-0.046401	2.455693
241.319483	1902.417788	18.064474	-0.046370	2.451109
241.210706	1894.437384	18.069479	-0.046345	2.446506
241.113734	1886.512148	18.074483	-0.046322	2.441928
241.055667	1878.557031	18.079488	-0.046306	2.437327
240.970802	1870.556115	18.084493	-0.046285	2.432689
241.022287	1862.528841	18.089498	-0.046289	2.428037
241.048595	1854.561565	18.094503	-0.046289	2.423409
241.038580	1846.635185	18.099507	-0.046282	2.418793
240.743876	1838.698864	18.104512	-0.046222	2.414140
240.694419	1830.731312	18.109517	-0.046208	2.409479
240.524740	1822.785602	18.114522	-0.046171	2.404813
240.467233	1814.835160	18.119527	-0.046155	2.400143
240.459526	1806.893045	18.124531	-0.046149	2.395474
240.686724	1798.857999	18.129536	-0.046186	2.390758
240.484561	1790.926994	18.134541	-0.046143	2.386061
240.542497	1782.972666	18.139546	-0.046149	2.381362
240.283465	1775.061776	18.144551	-0.046096	2.376653
240.135333	1767.105072	18.149555	-0.046063	2.371917
239.992175	1759.134583	18.154560	-0.046031	2.367164
240.160820	1751.159368	18.159565	-0.046057	2.362423
240.332265	1743.207757	18.164570	-0.046084	2.357687
239.843626	1735.283023	18.169575	-0.045988	2.352904
239.925700	1727.288914	18.174579	-0.045998	2.348117
239.731522	1719.351590	18.179584	-0.045957	2.343330
239.668669	1711.401645	18.184589	-0.045940	2.338538
239.704957	1703.427425	18.189594	-0.045942	2.333729
239.521821	1695.479092	18.194599	-0.045903	2.328907
239.389322	1687.539658	18.199603	-0.045873	2.324085
239.245022	1679.603493	18.204608	-0.045841	2.319254
239.341542	1671.636178	18.209613	-0.045854	2.314414
239.301540	1663.661939	18.214618	-0.045841	2.309548
239.208755	1655.693125	18.219623	-0.045819	2.304671
239.346423	1647.750859	18.224627	-0.045839	2.299819
239.102647	1639.822524	18.229632	-0.045789	2.294934
238.953852	1631.868487	18.234637	-0.045756	2.290029
238.963767	1623.914008	18.239642	-0.045753	2.285128
238.869685	1615.979061	18.244647	-0.045730	2.280219
238.965487	1608.037280	18.249651	-0.045743	2.275312
238.700309	1599.996091	18.254656	-0.045688	2.270301
238.952375	1592.019286	18.259661	-0.045730	2.265364
238.815853	1584.106349	18.264666	-0.045700	2.260423
238.593331	1576.191030	18.269671	-0.045653	2.255461
238.520373	1568.238816	18.274675	-0.045635	2.250479
238.370658	1560.277901	18.279680	-0.045602	2.245473
238.400724	1552.344720	18.284685	-0.045602	2.240489
238.269249	1544.419549	18.289690	-0.045573	2.235485
238.093869	1536.456111	18.294695	-0.045535	2.230441
238.142529	1528.502317	18.299699	-0.045539	2.225412
237.923512	1520.566150	18.304704	-0.045493	2.220359
237.881194	1512.632191	18.309709	-0.045480	2.215312
237.868833	1504.672470	18.314714	-0.045473	2.210240
237.822700	1496.713311	18.319719	-0.045459	2.205153
237.928662	1488.780309	18.324723	-0.045473	2.200084
237.837280	1480.852545	18.329728	-0.045451	2.194990
237.610638	1472.886721	18.334733	-0.045404	2.189847
237.635658	1464.928056	18.339738	-0.045404	2.184719
237.366790	1457.012835	18.344743	-0.045349	2.179580
237.357290	1449.081543	18.349747	-0.045342	2.174443
237.348059	1441.103379	18.354752	-0.045335	2.169263
237.312473	1433.162390	18.359757	-0.045323	2.164092
237.351667	1425.240958	18.364762	-0.045325	2.158929
237.024144	1417.332614	18.369767	-0.045259	2.153727
236.930842	1409.369427	18.374771	-0.045237	2.148499
236.936314	1401.412005	18.379776	-0.045233	2.143271
236.922716	1393.491149	18.384781	-0.045225	2.138053
236.746463	1385.567399	18.389786	-0.045187	2.132805
236.712930	1377.601291	18.394791	-0.045176	2.127529
236.657563	1369.683232	18.399795	-0.045160	2.122270
236.566500	1361.761373	18.404800	-0.045138	2.116992
236.836157	1353.736415	18.409805	-0.045183	2.111666
236.694048	1345.787958	18.414810	-0.045152	2.106338
236.490052	1337.886564	18.419815	-0.045109	2.101023
236.475597	1329.971103	18.424819	-0.045101	2.095703
236.370157	1322.032928	18.429824	-0.045076	2.090345
236.331742	1314.106578	18.434829	-0.045064	2.084988
236.069867	1306.207101	18.439834	-0.045010	2.079613
236.028958	1298.274906	18.444839	-0.044998	2.074224
236.137309	1290.303084	18.449843	-0.045013	2.068809
236.064348	1282.359093	18.454848	-0.044994	2.063380
235.968173	1274.460853	18.459853	-0.044971	2.057967
235.971851	1266.529513	18.464858	-0.044967	2.052526
236.027172	1258.559027	18.469863	-0.044972	2.047049
235.825366	1250.683043	18.474867	-0.044929	2.041596
235.616270	1242.778811	18.479872	-0.044885	2.036109
235.791004	1234.792988	18.484877	-0.044913	2.030589
235.601727	1226.877890	18.489882	-0.044872	2.025066
235.342290	1218.977871	18.494887	-0.044819	2.019531
235.626035	1211.022090	18.499891	-0.044867	2.013998
235.473969	1203.089264	18.504896	-0.044833	2.008421
235.210875	1195.201005	18.509901	-0.044779	2.002848
235.200932	1187.291357	18.514906	-0.044772	1.997270
234.935860	1179.377081	18.519911	-0.044718	1.991647
234.968719	1171.424535	18.524915	-0.044719	1.986012
234.936669	1163.498691	18.529920	-0.044708	1.980374
234.988155	1155.583398	18.534925	-0.044712	1.974735
234.872524	1147.660008	18.539930	-0.044686	1.969057
234.619037	1139.766455	18.544935	-0.044633	1.963369
234.787106	1131.843467	18.549939	-0.044660	1.957689
234.587434	1123.896866	18.554944	-0.044617	1.951935
234.471471	1115.955880	18.559949	-0.044591	1.946178
234.463235	1108.045254	18.564954	-0.044584	1.940437
234.693434	1100.088513	18.569959	-0.044622	1.934671
234.458392	1092.209558	18.574963	-0.044573	1.928894
234.288491	1084.304946	18.579968	-0.044536	1.923088
234.300445	1076.396849	18.584973	-0.044534	1.917282
234.100871	1068.489424	18.589978	-0.044491	1.911436
234.082684	1060.562197	18.594983	-0.044483	1.905577
234.216005	1052.649612	18.599987	-0.044503	1.899727
234.068190	1044.752142	18.604992	-0.044470	1.893840
233.838416	1036.857714	18.609997	-0.044422	1.887926
233.539889	1028.995727	18.615002	-0.044362	1.882011
233.651997	1021.050834	18.620007	-0.044377	1.876062
233.676398	1013.119135	18.625011	-0.044377	1.870093
233.424243	1005.227087	18.630016	-0.044325	1.864104
233.535632	997.315473	18.635021	-0.044340	1.858122
233.256209	989.444354	18.640026	-0.044283	1.852106
233.119623	981.519893	18.645031	-0.044253	1.846047
233.275599	973.609001	18.650035	-0.044277	1.840012
233.045045	965.735185	18.655040	-0.044229	1.833941
232.755963	957.839559	18.660045	-0.044170	1.827825
232.971536	949.899866	18.665050	-0.044205	1.821715
233.029268	942.003693	18.670055	-0.044211	1.815600
232.986624	934.110679	18.675059	-0.044198	1.809454
232.678557	926.249799	18.680064	-0.044135	1.803280
232.669495	918.365396	18.685069	-0.044129	1.797102
232.743969	910.409475	18.690074	-0.044137	1.790858
232.473396	902.517174	18.695079	-0.044082	1.784599
232.325222	894.662676	18.700083	-0.044049	1.778363
232.160454	886.765822	18.705088	-0.044014	1.772070
232.125455	878.866939	18.710093	-0.044002	1.765768
231.987976	871.002877	18.715098	-0.043971	1.759459
231.843366	863.125329	18.720103	-0.043939	1.753116
232.034104	855.192807	18.725107	-0.043970	1.746747
231.891214	847.325424	18.730112	-0.043938	1.740366
231.716688	839.477163	18.735117	-0.043901	1.733973
231.713570	831.578856	18.740122	-0.043895	1.727537
231.563610	823.710337	18.745127	-0.043862	1.721082
231.663390	815.829668	18.750131	-0.043875	1.714625
231.368533	807.959396	18.755136	-0.043816	1.708102
231.286968	800.078629	18.760141	-0.043795	1.701572
231.209271	792.223022	18.765146	-0.043776	1.695038
231.195984	784.325677	18.770151	-0.043768	1.688453
231.184271	776.457729	18.775155	-0.043761	1.681867
230.850207	768.636593	18.780160	-0.043694	1.675252
230.721112	760.757404	18.785165	-0.043665	1.668588
230.763159	752.866750	18.790170	-0.043667	1.661912
230.558895	745.019397	18.795175	-0.043624	1.655211
230.568372	737.152593	18.800179	-0.043621	1.648496
230.595735	729.273304	18.805184	-0.043621	1.641745
230.537690	721.431458	18.810189	-0.043605	1.634987
230.510925	713.507820	18.815194	-0.043595	1.628134
230.459681	705.646720	18.820199	-0.043581	1.621303
230.299989	697.834320	18.825203	-0.043546	1.614471
230.144907	689.976949	18.830208	-0.043512	1.607571
230.362740	682.095122	18.835213	-0.043548	1.600672
230.335102	674.263676	18.840218	-0.043537	1.593753
229.988508	666.437268	18.845223	-0.043468	1.586763
229.934951	658.615738	18.850227	-0.043453	1.579788
229.879523	650.759926	18.855232	-0.043438	1.572751
229.664766	642.938822	18.860237	-0.043393	1.565691
229.452051	635.147995	18.865242	-0.043348	1.558626
229.343227	627.293400	18.870247	-0.043323	1.551486
229.521522	619.405386	18.875251	-0.043351	1.544325
229.550412	611.568729	18.880256	-0.043351	1.537156
229.354588	603.749819	18.885261	-0.043310	1.529936
229.373123	595.915224	18.890266	-0.043308	1.522699
229.181881	588.119721	18.895271	-0.043267	1.515433
229.220963	580.275114	18.900275	-0.043270	1.508120
228.900022	572.492298	18.905280	-0.043205	1.500775
228.821652	564.679137	18.910285	-0.043185	1.493402
228.981862	556.816020	18.915290	-0.043210	1.485982
228.815653	549.038968	18.920295	-0.043174	1.478557
228.850902	541.189411	18.925299	-0.043176	1.471055
228.402142	533.413041	18.930304	-0.043087	1.463510
228.468346	525.589198	18.935309	-0.043095	1.455961
228.343262	517.799069	18.940314	-0.043066	1.448374
227.998131	510.033587	18.945319	-0.042997	1.440737
228.071695	502.232620	18.950323	-0.043006	1.433092
228.163565	494.396067	18.955328	-0.043018	1.425373
228.037592	486.635541	18.960333	-0.042989	1.417652
227.769144	478.870071	18.965338	-0.042934	1.409861
227.858364	471.056997	18.970343	-0.042946	1.402038
227.912248	463.279885	18.975347	-0.042951	1.394201
227.513201	455.529456	18.980352	-0.042872	1.386271
227.335977	447.770883	18.985357	-0.042834	1.378324
227.354149	439.987484	18.990362	-0.042832	1.370339
227.346772	432.205604	18.995367	-0.042826	1.362304
227.253392	424.466764	19.000371	-0.042803	1.354252
227.076720	416.707698	19.005376	-0.042766	1.346115
226.986833	408.966326	19.010381	-0.042744	1.337963
226.830219	401.225077	19.015386	-0.042710	1.329750
226.574704	393.499450	19.020391	-0.042657	1.321484
226.774611	385.701942	19.025395	-0.042689	1.313170
226.665767	377.867962	19.030400	-0.042664	1.304709
226.315303	370.196495	19.035405	-0.042594	1.296325
226.318819	362.460912	19.040410	-0.042590	1.287881
226.278182	354.735468	19.045415	-0.042577	1.279384
226.252597	347.035978	19.050419	-0.042568	1.270862
226.002594	339.352269	19.055424	-0.042516	1.262258
226.161907	331.618172	19.060429	-0.042541	1.253616
225.970868	323.937023	19.065434	-0.042500	1.244907
225.642701	316.294656	19.070439	-0.042434	1.236154
225.719597	308.567272	19.075443	-0.042444	1.227319
225.444134	300.912077	19.080448	-0.042387	1.218435
225.425164	293.223842	19.085453	-0.042379	1.209498
225.365227	285.556039	19.090458	-0.042363	1.200510
225.250318	277.897742	19.095463	-0.042337	1.191455
225.025622	270.266632	19.100467	-0.042290	1.182340
224.795337	262.638083	19.105472	-0.042242	1.173156
224.840628	254.969514	19.110477	-0.042246	1.163908
224.641812	247.362123	19.115482	-0.042204	1.154610
224.402955	239.712514	19.120487	-0.042154	1.145176
224.468887	232.074846	19.125491	-0.042162	1.135743
224.400982	224.445320	19.130496	-0.042144	1.126212
224.199144	216.870547	19.135501	-0.042102	1.116640
224.151652	209.265902	19.140506	-0.042088	1.106981
223.782424	201.727269	19.145511	-0.042014	1.097251
223.581393	194.164931	19.150515	-0.041972	1.087440
223.238056	186.639180	19.155520	-0.041903	1.077556
223.401993	179.013563	19.160525	-0.041929	1.067564
222.998721	171.519602	19.165530	-0.041849	1.057522
222.432835	164.033345	19.170535	-0.041739	1.047356
222.075211	156.554919	19.175539	-0.041668	1.037150
221.496257	149.096997	19.180544	-0.041555	1.026818
221.046809	141.633489	19.185549	-0.041467	1.016403
220.751190	134.145659	19.190554	-0.041407	1.005885
220.384914	126.680444	19.195559	-0.041334	0.995269
219.872765	119.226642	19.200563	-0.041234	0.984519
219.157551	111.840585	19.205568	-0.041096	0.973697
218.754562	104.411830	19.210573	-0.041016	0.962770
218.194189	97.038284	19.215578	-0.040907	0.951758
217.627744	89.659172	19.220583	-0.040797	0.940607
217.306441	82.267842	19.225587	-0.040732	0.929369
216.840383	74.916565	19.230592	-0.040641	0.918015
216.172392	67.597972	19.235597	-0.040512	0.906515
215.454760	60.550930	19.240602	-0.040373	0.895281