Thu Mar 11 21:01:33 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.721583	0.010829	0.000000	0.000020	0.721116

0.802862	0.040329	0.005005	0.000005	0.721203
1.003130	-0.040560	0.010010	-0.000032	0.721114
1.011734	-0.038234	0.015014	-0.000034	0.721122
1.000186	-0.037955	0.020019	-0.000032	0.721118
0.943181	-0.028588	0.025024	-0.000021	0.721117
1.058564	-0.046111	0.030029	-0.000043	0.721123
0.844868	-0.013564	0.035034	-0.000003	0.721112
0.858327	-0.009524	0.040038	-0.000006	0.721125
1.007897	-0.038848	0.045043	-0.000034	0.721120
0.925419	-0.023318	0.050048	-0.000018	0.721121
1.021119	-0.038566	0.055053	-0.000036	0.721125
0.912734	-0.023899	0.060058	-0.000016	0.721116
0.848774	-0.007025	0.065062	-0.000004	0.721127
0.796933	-0.003816	0.070067	0.000005	0.721115
0.745566	-0.111968	0.075072	0.000015	0.720884
0.796693	-0.124594	0.080077	0.000006	0.720877
0.750914	-0.122303	0.085082	0.000014	0.720866
0.937623	-0.151378	0.090086	-0.000021	0.720874
0.969344	-0.160350	0.095091	-0.000027	0.720868
0.953401	-0.157224	0.100096	-0.000024	0.720868
0.891937	-0.195768	0.105101	-0.000012	0.720771
0.868327	-0.315031	0.110106	-0.000008	0.720528
0.979300	-0.330186	0.115110	-0.000029	0.720537
0.905386	-0.317451	0.120115	-0.000015	0.720536
1.125537	-0.359501	0.125120	-0.000056	0.720531
1.148603	-0.433885	0.130125	-0.000060	0.720392
1.046362	-0.506508	0.135130	-0.000041	0.720214
1.096781	-0.509376	0.140134	-0.000050	0.720226
1.068985	-0.507706	0.145139	-0.000045	0.720219
0.945656	-0.558208	0.150144	-0.000022	0.720077
1.001963	-0.658352	0.155149	-0.000033	0.719899
0.941920	-0.651057	0.160154	-0.000022	0.719893
0.908010	-0.643861	0.165158	-0.000015	0.719895
0.930378	-0.760075	0.170163	-0.000020	0.719674
0.870701	-0.789114	0.175168	-0.000008	0.719596
1.032290	-0.815507	0.180173	-0.000039	0.719600
0.864328	-0.858432	0.185178	-0.000007	0.719457
0.784159	-0.940051	0.190182	0.000008	0.719268
1.057227	-0.991366	0.195187	-0.000043	0.719263
1.071042	-1.045302	0.200192	-0.000046	0.719161
1.009599	-1.135953	0.205197	-0.000034	0.718961
1.031688	-1.143439	0.210202	-0.000038	0.718954
0.863050	-1.195234	0.215206	-0.000007	0.718792
0.833907	-1.269996	0.220211	-0.000002	0.718635
0.766655	-1.258523	0.225216	0.000011	0.718634
0.809748	-1.375662	0.230221	0.000003	0.718418
0.619351	-1.379096	0.235226	0.000038	0.718344
0.735486	-1.420640	0.240230	0.000017	0.718303
0.741482	-1.569564	0.245235	0.000016	0.718011
0.630932	-1.552749	0.250240	0.000036	0.718005
0.669149	-1.653916	0.255245	0.000029	0.717819
0.811327	-1.741985	0.260250	0.000003	0.717695
0.929593	-1.804543	0.265254	-0.000019	0.717613
0.635946	-1.871337	0.270259	0.000035	0.717378
0.387903	-1.829042	0.275264	0.000082	0.717374
0.538645	-1.999373	0.280269	0.000054	0.717090
0.654657	-2.027408	0.285274	0.000032	0.717076
0.388689	-2.099592	0.290278	0.000081	0.716839
0.371352	-2.141653	0.295283	0.000085	0.716750
0.151643	-2.185711	0.300288	0.000126	0.716585
0.078160	-2.240067	0.305293	0.000139	0.716452
-0.119029	-2.260551	0.310298	0.000176	0.716342
0.079115	-2.400626	0.315302	0.000139	0.716134
-1.214612	-2.174887	0.320307	0.000380	0.716125
-1.631813	-2.226818	0.325312	0.000458	0.715875
-1.932507	-2.170762	0.330317	0.000513	0.715880
-2.461866	-2.118911	0.335322	0.000612	0.715796
-2.656145	-2.212025	0.340326	0.000648	0.715543
-2.651571	-2.211848	0.345331	0.000647	0.715545
-2.981963	-2.193528	0.350336	0.000709	0.715464
-3.432533	-2.230653	0.355341	0.000793	0.715232
-3.899420	-2.152035	0.360346	0.000879	0.715223
-4.414894	-2.057206	0.365350	0.000975	0.715229
-4.295591	-2.207453	0.370355	0.000953	0.714973
-4.942705	-2.128387	0.375360	0.001074	0.714901
-5.161295	-2.086958	0.380365	0.001114	0.714906
-4.876732	-2.141421	0.385370	0.001061	0.714899
-4.866169	-2.258867	0.390374	0.001059	0.714669
-5.801959	-2.123557	0.395379	0.001233	0.714607
-6.062906	-2.080126	0.400384	0.001282	0.714601
-5.481982	-2.180821	0.405389	0.001174	0.714607
-5.919942	-2.201607	0.410394	0.001255	0.714411
-6.965574	-2.082590	0.415398	0.001450	0.714277
-6.500329	-2.167512	0.420403	0.001363	0.714273
-6.635939	-2.144759	0.425408	0.001389	0.714270
-6.839472	-2.104127	0.430413	0.001426	0.714279
-7.059723	-2.176732	0.435418	0.001467	0.714057
-7.730601	-2.100838	0.440422	0.001592	0.713970
-7.799940	-2.089929	0.445427	0.001605	0.713967
-7.582894	-2.130279	0.450432	0.001565	0.713964
-7.493618	-2.141935	0.455437	0.001548	0.713973
-7.580902	-2.188585	0.460442	0.001564	0.713849
-8.637101	-2.101660	0.465446	0.001761	0.713648
-8.390613	-2.144861	0.470451	0.001715	0.713649
-8.529421	-2.122595	0.475456	0.001741	0.713645
-8.457100	-2.132213	0.480461	0.001727	0.713651
-8.563141	-2.117355	0.485466	0.001747	0.713643
-8.345467	-2.245979	0.490470	0.001707	0.713465
-9.635884	-2.069823	0.495475	0.001947	0.713358
-9.711951	-2.058381	0.500480	0.001961	0.713354
-9.278714	-2.132149	0.505485	0.001880	0.713361
-9.428381	-2.108927	0.510490	0.001908	0.713354
-9.270503	-2.133359	0.515494	0.001879	0.713361
-9.565776	-2.169573	0.520499	0.001934	0.713185
-10.692069	-2.053540	0.525504	0.002143	0.713016
-10.046969	-2.165295	0.530509	0.002023	0.713023
-10.427798	-2.101904	0.535514	0.002094	0.713014
-10.341731	-2.113701	0.540518	0.002078	0.713021
-9.998748	-2.175862	0.545523	0.002014	0.713019
-10.343647	-2.144640	0.550528	0.002078	0.712959
-10.800026	-2.187537	0.555533	0.002163	0.712712
-10.954289	-2.164904	0.560538	0.002192	0.712702
-11.555425	-2.055826	0.565542	0.002304	0.712706
-11.263615	-2.107342	0.570547	0.002249	0.712707
-10.926887	-2.168390	0.575552	0.002187	0.712705
-11.398690	-2.080357	0.580557	0.002274	0.712713
-11.675528	-2.127175	0.585562	0.002326	0.712521
-12.315339	-2.081784	0.590566	0.002445	0.712385
-11.751521	-2.183806	0.595571	0.002340	0.712382
-12.287243	-2.088890	0.600576	0.002440	0.712381
-12.539658	-2.041986	0.605581	0.002487	0.712385
-12.069033	-2.129361	0.610586	0.002399	0.712378
-11.904831	-2.154810	0.615590	0.002368	0.712385
-12.141656	-2.195549	0.620595	0.002413	0.712220
-13.500065	-2.023570	0.625600	0.002665	0.712081
-12.780773	-2.147421	0.630605	0.002531	0.712089
-13.237648	-2.070038	0.635610	0.002616	0.712081
-13.247630	-2.065236	0.640614	0.002618	0.712088
-13.130155	-2.086277	0.645619	0.002596	0.712087
-13.498775	-2.021957	0.650624	0.002665	0.712085
-13.094465	-2.127870	0.655629	0.002590	0.712017
-13.859182	-2.124142	0.660634	0.002732	0.711753
-14.052347	-2.087247	0.665638	0.002768	0.711758
-14.244928	-2.052492	0.670643	0.002804	0.711759
-13.953676	-2.107514	0.675648	0.002750	0.711753
-13.741669	-2.140272	0.680653	0.002710	0.711763
-14.569702	-1.998511	0.685658	0.002864	0.711752
-14.047747	-2.088965	0.690662	0.002767	0.711757
-14.290750	-2.188128	0.695667	0.002812	0.711473
-15.173634	-2.042339	0.700672	0.002976	0.711450
-14.968437	-2.075609	0.705677	0.002938	0.711456
-14.733785	-2.121406	0.710682	0.002895	0.711448
-14.948121	-2.079213	0.715686	0.002934	0.711456
-15.075753	-2.058535	0.720691	0.002958	0.711452
-14.944518	-2.084104	0.725696	0.002934	0.711448
-15.092184	-2.181884	0.730701	0.002961	0.711201
-16.015740	-2.052073	0.735706	0.003133	0.711131
-15.897441	-2.069977	0.740710	0.003111	0.711138
-15.492027	-2.143387	0.745715	0.003036	0.711135
-16.063356	-2.043407	0.750720	0.003142	0.711132
-15.863703	-2.074948	0.755725	0.003105	0.711140
-15.760399	-2.099606	0.760730	0.003085	0.711128
-16.060947	-2.137786	0.765734	0.003141	0.710945
-16.681743	-2.065782	0.770739	0.003257	0.710868
-16.494601	-2.100570	0.775744	0.003222	0.710865
-16.192122	-2.150124	0.780749	0.003166	0.710873
-16.763085	-2.052866	0.785754	0.003272	0.710865
-16.691473	-2.062061	0.790758	0.003259	0.710872
-16.105809	-2.184599	0.795763	0.003150	0.710836
-17.375914	-2.114640	0.800768	0.003386	0.710523
-17.356691	-2.112665	0.805773	0.003382	0.710534
-17.756622	-2.047249	0.810778	0.003457	0.710523
-17.218569	-2.139256	0.815782	0.003357	0.710530
-17.513305	-2.087545	0.820787	0.003411	0.710529
-17.956659	-2.010014	0.825792	0.003494	0.710526
-17.102013	-2.175008	0.830797	0.003335	0.710501
-18.119695	-2.141006	0.835802	0.003524	0.710206
-18.349704	-2.096962	0.840806	0.003567	0.710212
-18.602835	-2.051336	0.845811	0.003614	0.710214
-18.616606	-2.051998	0.850816	0.003617	0.710207
-18.259402	-2.110999	0.855821	0.003550	0.710217
-18.282215	-2.111730	0.860826	0.003554	0.710207
-18.059286	-2.179337	0.865830	0.003513	0.710152
-19.217829	-2.103443	0.870835	0.003728	0.709891
-19.456433	-2.064465	0.875840	0.003773	0.709884
-19.281061	-2.090830	0.880845	0.003740	0.709893
-19.324853	-2.088601	0.885850	0.003748	0.709882
-19.562086	-2.043543	0.890854	0.003792	0.709888
-19.177872	-2.111655	0.895859	0.003721	0.709889
-19.229832	-2.105393	0.900864	0.003730	0.709883
-19.746216	-2.135924	0.905869	0.003827	0.709638
-20.425100	-2.041503	0.910874	0.003953	0.709585
-20.085426	-2.098363	0.915878	0.003890	0.709592
-20.075707	-2.100204	0.920883	0.003888	0.709592
-20.507698	-2.026251	0.925888	0.003968	0.709586
-19.962070	-2.117513	0.930893	0.003867	0.709598
-20.072400	-2.102876	0.935898	0.003887	0.709588
-20.647028	-2.130188	0.940902	0.003994	0.709329
-21.276896	-2.051158	0.945907	0.004111	0.709262
-21.199582	-2.068908	0.950912	0.004097	0.709254
-21.017872	-2.097462	0.955917	0.004063	0.709262
-21.306140	-2.048574	0.960922	0.004117	0.709257
-21.039779	-2.093346	0.965926	0.004067	0.709263
-21.117114	-2.080063	0.970931	0.004081	0.709262
-21.587454	-2.048804	0.975936	0.004169	0.709156
-21.960602	-2.082075	0.980941	0.004238	0.708957
-21.922431	-2.093353	0.985946	0.004231	0.708948
-22.483387	-1.991068	0.990950	0.004336	0.708953
-21.912613	-2.091422	0.995955	0.004229	0.708955
-21.677630	-2.135555	1.000960	0.004186	0.708951
-22.134682	-2.049918	1.005965	0.004271	0.708959
-22.206264	-2.054189	1.010970	0.004284	0.708925
-22.439563	-2.157206	1.015974	0.004327	0.708636
-22.542928	-2.137840	1.020979	0.004347	0.708638
-23.479817	-1.973813	1.025984	0.004521	0.708632
-23.038803	-2.048237	1.030989	0.004439	0.708640
-22.908899	-2.076253	1.035994	0.004415	0.708631
-22.901090	-2.074947	1.040998	0.004413	0.708636
-22.911194	-2.073567	1.046003	0.004415	0.708635
-23.334039	-2.141726	1.051008	0.004494	0.708348
-23.452677	-2.117846	1.056013	0.004516	0.708354
-23.881203	-2.045901	1.061018	0.004595	0.708345
-23.901733	-2.040404	1.066022	0.004599	0.708348
-23.873643	-2.045597	1.071027	0.004594	0.708348
-24.242984	-1.983772	1.076032	0.004663	0.708340
-23.670205	-2.081606	1.081037	0.004556	0.708349
-24.037688	-2.168098	1.086042	0.004625	0.708044
-25.044650	-2.008117	1.091046	0.004812	0.708005
-24.933368	-2.027438	1.096051	0.004791	0.708006
-24.525987	-2.102415	1.101056	0.004715	0.708002
-24.652608	-2.075050	1.106061	0.004739	0.708011
-25.106502	-1.997061	1.111066	0.004823	0.708005
-24.591047	-2.087681	1.116070	0.004727	0.708008
-24.538986	-2.197540	1.121075	0.004718	0.707806
-26.041139	-1.988281	1.126080	0.004997	0.707689
-25.588371	-2.065472	1.131085	0.004913	0.707696
-25.275729	-2.123953	1.136090	0.004855	0.707691
-25.844605	-2.022237	1.141094	0.004961	0.707692
-25.689624	-2.048880	1.146099	0.004932	0.707694
-25.883233	-2.018994	1.151104	0.004968	0.707684
-25.758925	-2.101415	1.156109	0.004945	0.707564
-26.914213	-1.995576	1.161114	0.005160	0.707363
-26.403769	-2.083246	1.166118	0.005065	0.707370
-26.389196	-2.084397	1.171123	0.005062	0.707373
-26.801975	-2.015636	1.176128	0.005139	0.707363
-26.398414	-2.082660	1.181133	0.005063	0.707373
-26.463964	-2.075830	1.186138	0.005076	0.707363
-26.658528	-2.069535	1.191142	0.005112	0.707306
-27.396546	-2.052534	1.196147	0.005249	0.707076
-27.378741	-2.060870	1.201152	0.005246	0.707066
-27.341334	-2.060687	1.206157	0.005239	0.707080
-27.613502	-2.017648	1.211162	0.005289	0.707069
-27.682990	-2.002649	1.216166	0.005302	0.707074
-27.295733	-2.070891	1.221171	0.005230	0.707076
-27.583511	-2.022737	1.226176	0.005284	0.707070
-27.921779	-2.095215	1.231181	0.005347	0.706803
-28.350994	-2.050914	1.236186	0.005427	0.706739
-28.196232	-2.075967	1.241190	0.005398	0.706744
-28.022415	-2.104339	1.246195	0.005365	0.706749
-28.398264	-2.039395	1.251200	0.005435	0.706745
-28.237067	-2.063380	1.256205	0.005405	0.706755
-28.308427	-2.055198	1.261210	0.005419	0.706745
-28.940860	-2.082789	1.266214	0.005536	0.706464
-29.097115	-2.065687	1.271219	0.005565	0.706442
-29.419338	-2.012475	1.276224	0.005625	0.706434
-29.104001	-2.063201	1.281229	0.005567	0.706445
-28.962790	-2.090967	1.286234	0.005540	0.706440
-29.507209	-1.994340	1.291238	0.005642	0.706439
-29.184627	-2.049077	1.296243	0.005581	0.706444
-29.315478	-2.147338	1.301248	0.005606	0.706200
-30.183040	-2.027390	1.306253	0.005767	0.706130
-30.396232	-1.994658	1.311258	0.005807	0.706120
-30.250360	-2.018984	1.316262	0.005780	0.706123
-29.930670	-2.073712	1.321267	0.005720	0.706128
-30.350046	-2.001936	1.326272	0.005798	0.706122
-30.194597	-2.025795	1.331277	0.005769	0.706130
-30.349977	-2.057290	1.336282	0.005798	0.706011
-30.848148	-2.044318	1.341286	0.005891	0.705858
-30.703272	-2.069282	1.346291	0.005864	0.705860
-31.229487	-1.979118	1.351296	0.005962	0.705853
-30.975173	-2.019477	1.356301	0.005914	0.705863
-30.847514	-2.045835	1.361306	0.005891	0.705856
-30.764934	-2.058996	1.366310	0.005875	0.705859
-30.904257	-2.145825	1.371315	0.005901	0.705634
-32.101516	-1.993134	1.376320	0.006124	0.705512
-31.721463	-2.055758	1.381325	0.006053	0.705523
-31.723895	-2.057217	1.386330	0.006054	0.705519
-32.130229	-1.984928	1.391334	0.006129	0.705519
-32.111475	-1.987527	1.396339	0.006126	0.705520
-31.911367	-2.025441	1.401344	0.006088	0.705516
-31.773143	-2.131793	1.406349	0.006063	0.705351
-32.915755	-2.003276	1.411354	0.006275	0.705200
-32.821142	-2.017731	1.416358	0.006258	0.705205
-32.413360	-2.086465	1.421363	0.006182	0.705213
-32.836564	-2.018300	1.426368	0.006261	0.705199
-32.561207	-2.063077	1.431373	0.006209	0.705207
-32.702646	-2.039755	1.436378	0.006236	0.705204
-33.000814	-2.094513	1.441382	0.006291	0.704986
-33.802226	-2.002364	1.446387	0.006440	0.704884
-33.770135	-2.011100	1.451392	0.006434	0.704878
-33.407957	-2.070816	1.456397	0.006367	0.704888
-33.668144	-2.029228	1.461402	0.006415	0.704878
-33.652504	-2.030226	1.466406	0.006412	0.704882
-33.490661	-2.057250	1.471411	0.006382	0.704886
-33.811248	-2.081266	1.476416	0.006442	0.704722
-34.557253	-2.014544	1.481421	0.006581	0.704589
-34.049953	-2.109742	1.486426	0.006486	0.704579
-34.078279	-2.102670	1.491430	0.006491	0.704584
-34.307071	-2.059937	1.496435	0.006534	0.704588
-34.420008	-2.043319	1.501440	0.006555	0.704581
-34.214573	-2.075404	1.506445	0.006517	0.704590
-34.925618	-2.115114	1.511450	0.006649	0.704254
-35.490287	-2.012925	1.516454	0.006754	0.704257
-35.308458	-2.044677	1.521459	0.006720	0.704259
-35.375940	-2.036858	1.526464	0.006733	0.704250
-35.270696	-2.050542	1.531469	0.006713	0.704261
-35.364891	-2.037032	1.536474	0.006731	0.704254
-35.292797	-2.049993	1.541478	0.006717	0.704254
-35.565294	-2.138354	1.546483	0.006768	0.703978
-36.488073	-1.993060	1.551488	0.006940	0.703939
-36.316386	-2.017277	1.556493	0.006908	0.703952
-35.956464	-2.085347	1.561498	0.006841	0.703944
-36.292205	-2.025636	1.566502	0.006903	0.703944
-35.943894	-2.085793	1.571507	0.006838	0.703948
-35.991243	-2.091816	1.576512	0.006847	0.703919
-36.880438	-2.074876	1.581517	0.007013	0.703633
-37.045275	-2.048651	1.586522	0.007043	0.703627
-36.968690	-2.062104	1.591526	0.007029	0.703628
-36.937557	-2.064669	1.596531	0.007023	0.703634
-37.056918	-2.048370	1.601536	0.007045	0.703624
-37.091241	-2.038220	1.606541	0.007052	0.703632
-36.792512	-2.115764	1.611546	0.006996	0.703583
-37.815141	-2.056981	1.616550	0.007186	0.703334
-37.524091	-2.104651	1.621555	0.007132	0.703342
-37.931001	-2.037081	1.626560	0.007208	0.703332
-37.982497	-2.023910	1.631565	0.007217	0.703340
-37.906244	-2.038039	1.636570	0.007203	0.703339
-37.864207	-2.046841	1.641574	0.007195	0.703337
-37.610240	-2.154589	1.646579	0.007148	0.703211
-38.913685	-2.029512	1.651584	0.007391	0.702994
-38.608863	-2.077593	1.656589	0.007334	0.703007
-38.853612	-2.037000	1.661594	0.007379	0.703001
-39.070887	-1.998986	1.666598	0.007420	0.702999
-38.595580	-2.080634	1.671603	0.007331	0.703006
-38.911566	-2.027841	1.676608	0.007390	0.702998
-38.822620	-2.082953	1.681613	0.007374	0.702919
-39.575430	-2.063998	1.686618	0.007514	0.702686
-39.428048	-2.090347	1.691622	0.007486	0.702686
-39.640440	-2.049417	1.696627	0.007526	0.702693
-39.832255	-2.019419	1.701632	0.007561	0.702684
-39.459246	-2.082289	1.706637	0.007492	0.702692
-39.550425	-2.070543	1.711642	0.007509	0.702683
-39.854347	-2.082157	1.716646	0.007565	0.702550
-40.825141	-1.999405	1.721651	0.007746	0.702367
-40.430691	-2.073901	1.726656	0.007673	0.702359
-40.526499	-2.051212	1.731661	0.007691	0.702370
-40.810150	-2.005028	1.736666	0.007743	0.702361
-40.463508	-2.067215	1.741670	0.007679	0.702361
-40.244546	-2.102853	1.746675	0.007638	0.702368
-40.496970	-2.100186	1.751680	0.007685	0.702282
-41.263403	-2.068268	1.756685	0.007828	0.702070
-41.285131	-2.067281	1.761690	0.007832	0.702064
-41.751158	-1.983790	1.766694	0.007918	0.702065
-41.281813	-2.064770	1.771699	0.007831	0.702071
-41.223609	-2.078421	1.776704	0.007820	0.702064
-41.511541	-2.024255	1.781709	0.007874	0.702070
-41.318389	-2.109933	1.786714	0.007838	0.701967
-42.313999	-2.047936	1.791718	0.008023	0.701733
-41.929809	-2.110996	1.796723	0.007951	0.701744
-42.794606	-1.962144	1.801728	0.008112	0.701733
-42.152951	-2.072542	1.806733	0.007993	0.701741
-41.765697	-2.144441	1.811738	0.007921	0.701736
-42.319357	-2.045978	1.816742	0.008024	0.701735
-42.322063	-2.112364	1.821747	0.008024	0.701600
-43.032143	-2.073072	1.826752	0.008156	0.701423
-42.672900	-2.132305	1.831757	0.008090	0.701433
-42.986794	-2.077713	1.836762	0.008148	0.701430
-43.249599	-2.029223	1.841766	0.008197	0.701434
-42.719948	-2.121734	1.846771	0.008098	0.701438
-43.283522	-2.026706	1.851776	0.008203	0.701427
-43.502614	-2.107394	1.856781	0.008244	0.701184
-43.804988	-2.088112	1.861786	0.008300	0.701114
-44.233305	-2.012111	1.866790	0.008380	0.701113
-43.757943	-2.093711	1.871795	0.008291	0.701120
-44.084249	-2.040564	1.876800	0.008352	0.701110
-44.010865	-2.049751	1.881805	0.008338	0.701118
-43.952799	-2.061138	1.886810	0.008327	0.701116
-44.439007	-2.071524	1.891814	0.008418	0.700919
-44.517957	-2.081437	1.896819	0.008433	0.700871
-44.736348	-2.046530	1.901824	0.008473	0.700862
-44.812674	-2.029483	1.906829	0.008487	0.700869
-44.694551	-2.051426	1.911834	0.008465	0.700868
-44.840117	-2.025884	1.916838	0.008492	0.700867
-44.676833	-2.063161	1.921843	0.008462	0.700850
-45.368543	-2.101126	1.926848	0.008591	0.700524
-44.982563	-2.165714	1.931853	0.008519	0.700532
-45.611529	-2.055353	1.936858	0.008636	0.700529
-45.748204	-2.032436	1.941862	0.008661	0.700526
-45.404039	-2.088875	1.946867	0.008597	0.700536
-45.739139	-2.034576	1.951872	0.008660	0.700525
-45.764228	-2.111054	1.956877	0.008664	0.700361
-46.667011	-2.023832	1.961882	0.008832	0.700211
-46.528529	-2.050176	1.966886	0.008807	0.700208
-46.345912	-2.077809	1.971891	0.008773	0.700218
-46.785266	-2.005492	1.976896	0.008854	0.700206
-46.485437	-2.053913	1.981901	0.008798	0.700216
-46.610193	-2.032657	1.986906	0.008822	0.700214
-46.641149	-2.085081	1.991910	0.008827	0.700097
-47.047163	-2.112846	1.996915	0.008903	0.699894
-47.403103	-2.050526	2.001920	0.008969	0.699891

-47.116228	-2.101902	2.011917	0.008916	0.699891
-47.648480	-2.007698	2.021914	0.009015	0.699890
-47.222671	-2.082542	2.031910	0.008935	0.699892
-47.555530	-2.023551	2.041907	0.008997	0.699891
-47.459898	-2.116186	2.051904	0.008979	0.699738
-47.672618	-2.009534	2.061901	0.009019	0.699878
-47.630258	-2.053274	2.071898	0.009011	0.699804
-47.191651	-2.089501	2.081894	0.008929	0.699890
-47.498603	-2.035245	2.091891	0.008986	0.699889
-47.659487	-2.005768	2.101888	0.009016	0.699891
-47.397688	-2.053828	2.111885	0.008967	0.699888
-47.668568	-2.004234	2.121882	0.009018	0.699891
-47.341649	-2.063214	2.131878	0.008957	0.699889
-47.409651	-1.959395	2.141875	0.008969	0.700076
-46.366626	-2.079079	2.151872	0.008775	0.700210
-46.716592	-2.016962	2.161869	0.008840	0.700210
-46.321144	-2.086890	2.171866	0.008767	0.700211
-46.409843	-2.071057	2.181862	0.008783	0.700211
-45.863825	-2.050791	2.191859	0.008681	0.700450
-45.799448	-2.023746	2.201856	0.008669	0.700528
-45.566895	-2.065047	2.211853	0.008626	0.700529
-45.767412	-2.029081	2.221850	0.008663	0.700529
-44.873421	-2.082071	2.231846	0.008497	0.700745
-44.734002	-2.045172	2.241843	0.008471	0.700870
-44.747776	-2.044397	2.251840	0.008473	0.700867
-44.669753	-2.058218	2.261837	0.008459	0.700867
-44.475728	-2.030351	2.271834	0.008422	0.700994
-43.862567	-2.078061	2.281830	0.008308	0.701119
-44.197551	-2.019083	2.291827	0.008370	0.701118
-43.991464	-2.049682	2.301824	0.008332	0.701130
-43.329622	-2.019021	2.311821	0.008209	0.701431
-43.099062	-2.059617	2.321818	0.008166	0.701432
-43.124212	-2.053804	2.331814	0.008170	0.701435
-43.070196	-1.969718	2.341811	0.008160	0.701625
-42.472735	-2.019356	2.351808	0.008049	0.701740
-42.452898	-2.024654	2.361805	0.008045	0.701737
-42.297344	-1.990462	2.371802	0.008016	0.701862
-41.667568	-1.999977	2.381798	0.007899	0.702070
-41.517311	-2.028222	2.391795	0.007871	0.702068
-41.465826	-2.027573	2.401792	0.007861	0.702088
-40.896451	-1.993270	2.411789	0.007755	0.702362
-40.666202	-2.033923	2.421786	0.007712	0.702363
-40.678957	-2.030165	2.431782	0.007714	0.702366
-40.157699	-2.016266	2.441779	0.007617	0.702583
-39.857181	-2.019676	2.451776	0.007561	0.702684
-39.940724	-2.006002	2.461773	0.007577	0.702682
-39.617329	-2.016655	2.471770	0.007516	0.702777
-38.901505	-2.033163	2.481766	0.007383	0.703001
-38.948047	-2.025390	2.491763	0.007392	0.703001
-39.031738	-2.010762	2.501760	0.007407	0.703000
-38.453558	-1.979852	2.511757	0.007299	0.703271
-37.910066	-2.044299	2.521754	0.007198	0.703336
-38.031353	-2.023433	2.531750	0.007221	0.703335
-38.005729	-1.986367	2.541747	0.007216	0.703419
-37.154651	-2.034391	2.551744	0.007057	0.703629
-37.098765	-2.045036	2.561741	0.007047	0.703627
-37.091710	-2.046279	2.571738	0.007046	0.703627
-36.782972	-1.981186	2.581734	0.006988	0.703870
-36.332267	-2.021927	2.591731	0.006904	0.703950
-36.327918	-2.024005	2.601728	0.006903	0.703948
-36.265806	-1.980191	2.611725	0.006891	0.704058
-35.355694	-2.044643	2.621722	0.006722	0.704256
-35.622492	-1.996674	2.631718	0.006772	0.704257
-35.463482	-2.025434	2.641715	0.006742	0.704256
-34.933126	-1.963282	2.651712	0.006643	0.704572
-34.516246	-2.032468	2.661709	0.006565	0.704582
-34.388707	-2.055461	2.671706	0.006542	0.704582
-34.272131	-2.013741	2.681702	0.006520	0.704708
-33.429164	-2.077839	2.691699	0.006363	0.704882
-33.667069	-2.036031	2.701696	0.006407	0.704881
-33.648299	-2.039051	2.711693	0.006403	0.704881
-32.836015	-2.067419	2.721690	0.006252	0.705116
-33.165243	-1.963526	2.731686	0.006313	0.705207
-32.510614	-2.080523	2.741683	0.006191	0.705207
-32.794357	-1.993198	2.751680	0.006244	0.705281
-31.852092	-2.044470	2.761677	0.006069	0.705516
-32.082330	-2.003798	2.771674	0.006111	0.705515
-32.057787	-2.007575	2.781670	0.006107	0.705516
-31.409365	-1.975222	2.791667	0.005986	0.705814
-30.837240	-2.056913	2.801664	0.005879	0.705855
-30.929590	-2.039890	2.811661	0.005897	0.705856
-30.876023	-2.017519	2.821658	0.005887	0.705921
-30.269870	-2.023957	2.831654	0.005774	0.706125
-30.004944	-2.072683	2.841651	0.005724	0.706122
-30.412629	-2.000615	2.851648	0.005800	0.706121
-29.467236	-2.033001	2.861645	0.005624	0.706395
-29.449836	-2.015553	2.871642	0.005621	0.706436
-29.112332	-2.074066	2.881638	0.005558	0.706440
-29.277903	-1.989927	2.891635	0.005588	0.706550
-28.258264	-2.074757	2.901632	0.005399	0.706745
-28.537518	-2.023407	2.911629	0.005451	0.706748
-28.491750	-2.032444	2.921626	0.005442	0.706746
-27.739469	-2.020153	2.931622	0.005302	0.707040
-27.510696	-2.042152	2.941619	0.005259	0.707078
-27.719512	-2.006161	2.951616	0.005298	0.707076
-27.224741	-2.035589	2.961613	0.005206	0.707194
-26.696722	-2.041139	2.971610	0.005107	0.707372
-26.693411	-2.040857	2.981606	0.005107	0.707374
-26.692206	-2.040199	2.991603	0.005106	0.707375
-25.950603	-2.023797	3.001600	0.004968	0.707674
-25.911064	-2.022100	3.011597	0.004961	0.707691
-25.716898	-2.055796	3.021594	0.004925	0.707693
-25.818356	-1.969659	3.031590	0.004943	0.707830
-24.894927	-2.044859	3.041587	0.004771	0.708009
-25.074559	-2.012903	3.051584	0.004805	0.708009
-25.005506	-2.007497	3.061581	0.004792	0.708045
-24.256800	-1.990063	3.071578	0.004652	0.708347
-23.818134	-2.067724	3.081574	0.004571	0.708349
-24.017150	-2.031769	3.091571	0.004608	0.708350
-23.947357	-1.967584	3.101568	0.004595	0.708503
-23.199052	-2.035472	3.111565	0.004455	0.708635
-23.333599	-2.010851	3.121562	0.004480	0.708636
-23.100581	-2.032232	3.131558	0.004437	0.708676
-22.299181	-2.037588	3.141555	0.004287	0.708952
-22.262209	-2.043653	3.151552	0.004281	0.708953
-22.229513	-2.051260	3.161549	0.004274	0.708950
-22.233962	-1.968699	3.171546	0.004275	0.709113
-21.400417	-2.042848	3.181542	0.004120	0.709262
-21.492595	-2.026131	3.191539	0.004137	0.709263
-21.553445	-1.996406	3.201536	0.004148	0.709301
-20.782054	-1.989639	3.211533	0.004004	0.709590
-20.609003	-2.019369	3.221530	0.003972	0.709592
-20.577587	-2.025616	3.231526	0.003966	0.709591
-20.256421	-1.970052	3.241523	0.003906	0.709817
-19.740842	-2.025528	3.251520	0.003810	0.709890
-19.723088	-2.029692	3.261517	0.003807	0.709888
-19.721359	-1.985809	3.271514	0.003807	0.709976
-18.667856	-2.054471	3.281510	0.003610	0.710214
-18.916638	-2.010549	3.291507	0.003657	0.710214
-18.891422	-2.013384	3.301504	0.003652	0.710217
-18.249077	-2.004269	3.311501	0.003532	0.710464
-18.073730	-2.001422	3.321498	0.003499	0.710532
-17.759476	-2.056351	3.331494	0.003441	0.710534
-18.026983	-1.973447	3.341491	0.003491	0.710605
-16.898632	-2.043467	3.351488	0.003281	0.710867
-17.039991	-2.016694	3.361485	0.003307	0.710870
-16.866748	-2.047628	3.371482	0.003274	0.710870
-16.679172	-2.011584	3.381478	0.003239	0.711009
-16.118205	-2.045939	3.391475	0.003135	0.711140
-16.107423	-2.047061	3.401472	0.003133	0.711142
-16.156502	-2.040962	3.411469	0.003142	0.711136
-15.658974	-1.980635	3.421466	0.003049	0.711434
-14.955161	-2.095925	3.431462	0.002918	0.711454
-15.396546	-2.018628	3.441459	0.003000	0.711452
-14.960653	-2.037195	3.451456	0.002919	0.711570
-14.426186	-2.039528	3.461453	0.002819	0.711755
-14.240040	-2.071544	3.471450	0.002785	0.711757
-14.446642	-2.034831	3.481446	0.002823	0.711757
-13.716949	-2.020085	3.491443	0.002687	0.712046
-13.666929	-2.007570	3.501440	0.002678	0.712089
-13.702965	-2.003132	3.511437	0.002684	0.712085
-13.463033	-1.968287	3.521434	0.002640	0.712240
-12.554418	-2.058811	3.531430	0.002470	0.712382
-12.940090	-1.988348	3.541427	0.002542	0.712386
-12.592217	-2.026029	3.551424	0.002477	0.712434
-12.035411	-1.988846	3.561421	0.002374	0.712706
-11.670807	-2.053088	3.571418	0.002306	0.712707
-11.950195	-2.005410	3.581414	0.002358	0.712703
-11.180328	-2.029302	3.591411	0.002214	0.712929
-11.102065	-1.996932	3.601408	0.002200	0.713021
-10.877443	-2.037605	3.611405	0.002158	0.713020
-10.903348	-2.007681	3.621402	0.002162	0.713071
-10.213220	-1.986419	3.631398	0.002034	0.713358
-9.732842	-2.071442	3.641395	0.001944	0.713359
-9.702564	-2.076544	3.651392	0.001939	0.713360
-9.813871	-2.003570	3.661389	0.001959	0.713465
-8.599155	-2.128402	3.671386	0.001733	0.713648
-8.847449	-2.082654	3.681382	0.001779	0.713651
-8.759477	-2.097092	3.691379	0.001763	0.713653
-8.573128	-2.059553	3.701376	0.001728	0.713794
-7.831189	-2.104548	3.711373	0.001590	0.713968
-8.000408	-2.075129	3.721370	0.001621	0.713966
-7.922723	-2.087773	3.731366	0.001607	0.713969
-7.477296	-2.068391	3.741363	0.001524	0.714165
-6.946225	-2.109761	3.751360	0.001425	0.714271
-7.245844	-2.055223	3.761357	0.001481	0.714273
-6.887166	-2.118597	3.771354	0.001414	0.714274
-6.308492	-2.073669	3.781350	0.001306	0.714569
-6.023407	-2.105469	3.791347	0.001253	0.714606
-5.997932	-2.111092	3.801344	0.001248	0.714604
-5.808594	-2.144453	3.811341	0.001213	0.714605
-5.418963	-2.062858	3.821338	0.001140	0.714905
-5.224987	-2.096768	3.831334	0.001104	0.714906
-5.177668	-2.104748	3.841331	0.001095	0.714908
-5.050236	-2.042990	3.851328	0.001071	0.715075
-4.265381	-2.107155	3.861325	0.000925	0.715225
-4.323650	-2.095418	3.871322	0.000936	0.715228
-4.185581	-2.119762	3.881318	0.000910	0.715229
-3.442399	-2.122766	3.891315	0.000772	0.715486
-3.487616	-2.087142	3.901312	0.000780	0.715540
-3.263246	-2.126622	3.911309	0.000738	0.715541
-3.500050	-2.054895	3.921306	0.000782	0.715600
-2.458847	-2.099243	3.931302	0.000588	0.715880
-2.294061	-2.128738	3.941299	0.000557	0.715880
-2.529923	-2.087021	3.951296	0.000601	0.715879
-2.105479	-2.108501	3.961293	0.000522	0.715987
-1.879725	-2.076156	3.971290	0.000480	0.716131
-1.729067	-2.103331	3.981286	0.000452	0.716130
-1.997508	-2.018409	3.991283	0.000502	0.716204
-1.329408	-2.015899	4.001280	0.000377	0.716444
-1.204480	-2.038332	4.011277	0.000354	0.716444
-1.353576	-1.963443	4.021274	0.000382	0.716540
-0.896873	-1.938773	4.031270	0.000297	0.716750
-0.857381	-1.943303	4.041267	0.000289	0.716755
-0.833257	-1.841545	4.051264	0.000284	0.716965
-0.845336	-1.781468	4.061261	0.000287	0.717080
-1.050959	-1.683389	4.071258	0.000325	0.717202
-0.819845	-1.635785	4.081254	0.000282	0.717377
-0.603672	-1.598898	4.091251	0.000241	0.717526
-0.744734	-1.485950	4.101248	0.000267	0.717700
-0.614803	-1.405191	4.111245	0.000243	0.717906
-0.546471	-1.362722	4.121242	0.000230	0.718014
-0.522580	-1.200666	4.131238	0.000226	0.718342
-0.376419	-1.163356	4.141235	0.000198	0.718467
-0.299835	-1.091156	4.151232	0.000184	0.718637
-0.417619	-0.923922	4.161229	0.000206	0.718926
-0.192674	-0.867908	4.171226	0.000164	0.719116
-0.234934	-0.756195	4.181222	0.000172	0.719321
-0.088642	-0.642275	4.191219	0.000144	0.719597
-0.000437	-0.525254	4.201216	0.000128	0.719859
-0.071632	-0.390944	4.211213	0.000141	0.720099
-0.136645	-0.247496	4.221210	0.000153	0.720359
-0.127639	-0.102532	4.231206	0.000151	0.720647
-0.088462	0.037317	4.241203	0.000143	0.720936
0.000000	0.181136	4.251200	0.000127	0.721250

0.041931	0.815381	4.256205	0.000118	0.722511
0.167893	2.057713	4.261210	0.000094	0.724990
0.287855	3.895276	4.266214	0.000071	0.728619
0.682707	6.236919	4.271219	-0.000004	0.733299
0.910160	9.112384	4.276224	-0.000049	0.738918
1.220049	12.458852	4.281229	-0.000109	0.745420
1.516557	16.255143	4.286234	-0.000166	0.752709
2.009012	20.425624	4.291238	-0.000261	0.760690
2.386757	25.019462	4.296243	-0.000334	0.769332
2.655966	29.994608	4.301248	-0.000388	0.778538
3.278508	35.259381	4.306253	-0.000507	0.788270
3.830145	40.851165	4.311258	-0.000613	0.798442
4.431364	46.742060	4.316262	-0.000729	0.809026
5.272565	52.882212	4.321267	-0.000890	0.819978
6.254454	59.265505	4.326272	-0.001077	0.831242
7.344559	65.877237	4.331277	-0.001284	0.842771
7.893753	72.802417	4.336282	-0.001391	0.854507
8.924276	79.850976	4.341286	-0.001587	0.866423
9.695248	87.141282	4.346291	-0.001736	0.878495
10.259500	94.634429	4.351296	-0.001846	0.890667
11.155253	102.243290	4.356301	-0.002018	0.902948
11.950622	110.009905	4.361306	-0.002171	0.915281
12.940981	117.859835	4.366310	-0.002360	0.927628
13.689941	125.884501	4.371315	-0.002505	0.940013
14.405540	134.010159	4.376320	-0.002644	0.952379
15.354834	142.192307	4.381325	-0.002826	0.964728
15.824231	150.536938	4.386330	-0.002919	0.977035
16.792810	158.882745	4.391334	-0.003104	0.989315
17.558100	167.310697	4.396339	-0.003252	1.001510
18.357962	175.767159	4.401344	-0.003407	1.013606
19.193630	184.273009	4.406349	-0.003568	1.025635
19.800975	192.842044	4.411354	-0.003687	1.037557
20.226216	201.457452	4.416358	-0.003772	1.049364
20.839815	210.067176	4.421363	-0.003892	1.061074
21.480501	218.692152	4.426368	-0.004016	1.072683
22.396375	227.276773	4.431373	-0.004193	1.084177
22.916450	235.943908	4.436378	-0.004295	1.095567
23.785144	244.548106	4.441382	-0.004463	1.106837
24.559942	253.194021	4.446387	-0.004612	1.118025
25.536320	261.782626	4.451392	-0.004800	1.129073
26.143598	270.459655	4.456397	-0.004919	1.140045
26.653374	279.148393	4.461402	-0.005019	1.150906
27.226212	287.802584	4.466406	-0.005132	1.161636
28.119504	296.382361	4.471411	-0.005304	1.172243
28.649181	305.002672	4.476416	-0.005408	1.182730
29.405336	313.604453	4.481421	-0.005554	1.193147
30.232047	322.159059	4.486426	-0.005714	1.203433
31.043916	330.729836	4.491430	-0.005871	1.213647
31.780637	339.298374	4.496435	-0.006013	1.223758
32.215103	347.912884	4.501440	-0.006100	1.233780
32.926406	356.445476	4.506445	-0.006238	1.243680
33.535860	364.981792	4.511450	-0.006357	1.253487
34.104047	373.507291	4.516454	-0.006468	1.263198
34.856315	382.004162	4.521459	-0.006614	1.272837
35.547163	390.475917	4.526464	-0.006748	1.282364
36.506513	398.926908	4.531469	-0.006932	1.291847
37.138196	407.394940	4.536474	-0.007056	1.301219
37.874459	415.916185	4.541478	-0.007198	1.310601
38.287895	424.466317	4.546483	-0.007281	1.319888
38.690308	432.906808	4.551488	-0.007361	1.328991
39.217037	441.340204	4.556493	-0.007465	1.338047
39.516347	449.772946	4.561498	-0.007526	1.347001
39.996643	458.182907	4.566502	-0.007621	1.355903
40.561608	466.548146	4.571507	-0.007732	1.364715
41.061746	474.935645	4.576512	-0.007830	1.373483
41.599610	483.309057	4.581517	-0.007936	1.382186
42.100489	491.679480	4.586522	-0.008035	1.390826
42.587664	500.044943	4.591526	-0.008131	1.399404
43.255053	508.364920	4.596531	-0.008261	1.407915
43.799855	516.705083	4.601536	-0.008368	1.416374
44.270510	525.051250	4.606541	-0.008461	1.424776
44.641139	533.405377	4.611546	-0.008535	1.433120
45.168355	541.708041	4.616550	-0.008639	1.441391
45.616039	550.025985	4.621555	-0.008728	1.449616
45.831597	558.376399	4.626560	-0.008773	1.457790
46.428630	566.645675	4.631565	-0.008890	1.465899
46.962006	574.970929	4.636570	-0.008995	1.474008
47.606958	583.214479	4.641574	-0.009120	1.482011
48.503387	591.435934	4.646579	-0.009292	1.489990
48.742660	599.755456	4.651584	-0.009342	1.497916
49.202616	608.026173	4.656589	-0.009434	1.505789
49.866352	616.277263	4.661594	-0.009563	1.513633
50.205243	624.556223	4.666598	-0.009631	1.521414
50.677858	632.820762	4.671603	-0.009724	1.529161
51.234704	641.062540	4.676608	-0.009834	1.536861
51.912046	649.286862	4.681613	-0.009965	1.544524
52.075904	657.604643	4.686618	-0.010001	1.552158
52.483078	665.845038	4.691622	-0.010082	1.559721
52.914051	674.072048	4.696627	-0.010168	1.567238
53.446266	682.283574	4.701632	-0.010272	1.574720
54.023990	690.491414	4.706637	-0.010385	1.582169
54.330290	698.745066	4.711642	-0.010448	1.589586
54.767725	706.983155	4.716646	-0.010535	1.596972
55.172508	715.199425	4.721651	-0.010615	1.604301
55.369554	723.448569	4.726656	-0.010658	1.611596
56.012496	731.635564	4.731661	-0.010783	1.618866
56.407778	739.841886	4.736666	-0.010862	1.626085
56.833412	748.116865	4.741670	-0.010946	1.633336
57.368038	756.285010	4.746675	-0.011051	1.640478
57.565781	764.490435	4.751680	-0.011093	1.647575
57.980930	772.697803	4.756685	-0.011176	1.654672
58.721054	780.815061	4.761690	-0.011319	1.661706
59.000422	789.023815	4.766694	-0.011377	1.668725
59.509764	797.212351	4.771699	-0.011477	1.675729
59.860080	805.380068	4.776704	-0.011547	1.682665
60.469744	813.547572	4.781709	-0.011666	1.689607
60.859056	821.738733	4.786714	-0.011744	1.696510
61.250842	829.923144	4.791718	-0.011822	1.703380
61.923132	838.075910	4.796723	-0.011953	1.710233
62.092425	846.311585	4.801728	-0.011990	1.717061
62.440700	854.478587	4.806733	-0.012060	1.723829
62.733350	862.650192	4.811738	-0.012120	1.730567
63.071468	870.836318	4.816742	-0.012188	1.737297
63.646405	878.967684	4.821747	-0.012301	1.743985
63.698815	887.174222	4.826752	-0.012316	1.750643
64.044327	895.354096	4.831757	-0.012385	1.757291
64.964402	903.411899	4.836762	-0.012562	1.763888
65.436500	911.572573	4.841766	-0.012655	1.770486
65.965547	919.731038	4.846771	-0.012759	1.777065
66.783077	927.818428	4.851776	-0.012917	1.783599
67.183423	936.022379	4.856781	-0.012997	1.790150
67.757260	944.207723	4.861786	-0.013109	1.796683
67.935237	952.375415	4.866790	-0.013147	1.803130
68.206606	960.535359	4.871795	-0.013203	1.809559
68.348401	968.707192	4.876800	-0.013235	1.815960
68.918429	976.828305	4.881805	-0.013346	1.822349
69.115896	984.994555	4.886810	-0.013389	1.828707
69.234411	993.180547	4.891814	-0.013416	1.835048
69.868663	1001.273729	4.896819	-0.013539	1.841358
70.391678	1009.364894	4.901824	-0.013642	1.847630
71.038856	1017.494470	4.906829	-0.013768	1.853925
71.181303	1025.658190	4.911834	-0.013800	1.860166
71.554330	1033.789133	4.916838	-0.013875	1.866388
72.002493	1041.946842	4.921843	-0.013963	1.872618
72.203614	1050.094625	4.926848	-0.014006	1.878791
72.615800	1058.194049	4.931853	-0.014088	1.884932
72.975729	1066.324892	4.936858	-0.014161	1.891071
73.438314	1074.445157	4.941862	-0.014252	1.897193
73.889149	1082.550430	4.946867	-0.014341	1.903282
74.172030	1090.691952	4.951872	-0.014399	1.909361
74.638126	1098.823315	4.956877	-0.014491	1.915433
74.911413	1106.936741	4.961882	-0.014548	1.921450
75.266074	1115.056786	4.966886	-0.014619	1.927463
75.850615	1123.174274	4.971891	-0.014733	1.933481
75.790695	1131.337156	4.976896	-0.014727	1.939442
76.263189	1139.450038	4.981901	-0.014821	1.945406
76.890529	1147.553387	4.986906	-0.014943	1.951362
77.407185	1155.661309	4.991910	-0.015044	1.957292
77.870302	1163.747307	4.996915	-0.015136	1.963181
78.184352	1171.849673	5.001920	-0.015200	1.969049
78.442981	1179.996748	5.006925	-0.015253	1.974925
78.659221	1188.109994	5.011930	-0.015299	1.980755
79.078266	1196.190418	5.016934	-0.015382	1.986565
79.752051	1204.289504	5.021939	-0.015513	1.992399
79.901521	1212.418728	5.026944	-0.015546	1.998182
80.280501	1220.518157	5.031949	-0.015622	2.003951
80.570904	1228.632882	5.036954	-0.015681	2.009705
80.846133	1236.764034	5.041958	-0.015738	2.015453
81.236626	1244.867509	5.046963	-0.015816	2.021176
81.375125	1252.980061	5.051968	-0.015847	2.026864
81.887367	1261.104624	5.056973	-0.015948	2.032582
82.166594	1269.204742	5.061978	-0.016005	2.038244
82.388270	1277.295734	5.066982	-0.016052	2.043877
83.057327	1285.349694	5.071987	-0.016181	2.049515
83.453831	1293.451823	5.076992	-0.016261	2.055143
83.859502	1301.530153	5.081997	-0.016341	2.060740
84.413168	1309.601178	5.087002	-0.016450	2.066331
84.643680	1317.749688	5.092006	-0.016498	2.071928
84.912465	1325.871319	5.097011	-0.016553	2.077495
85.202896	1333.930942	5.102016	-0.016613	2.083007
85.774281	1342.003105	5.107021	-0.016724	2.088541
85.965653	1350.146074	5.112026	-0.016765	2.094070
86.183099	1358.251606	5.117030	-0.016811	2.099563
86.557853	1366.344164	5.122035	-0.016886	2.105047
86.500629	1374.500108	5.127040	-0.016881	2.110518
86.924905	1382.622367	5.132045	-0.016965	2.115998
87.365397	1390.647627	5.137050	-0.017053	2.121401
87.938737	1398.688644	5.142054	-0.017165	2.126814
88.194945	1406.808903	5.147059	-0.017218	2.132235
88.535642	1414.874949	5.152064	-0.017286	2.137614
89.122394	1422.927719	5.157069	-0.017401	2.142994
89.222254	1431.052193	5.162074	-0.017425	2.148362
89.603694	1439.143265	5.167078	-0.017501	2.153721
90.068768	1447.216650	5.172083	-0.017593	2.159063
90.219115	1455.289862	5.177088	-0.017626	2.164362
90.649349	1463.375194	5.182093	-0.017712	2.169681
90.995123	1471.478323	5.187098	-0.017781	2.174992
91.048240	1479.595234	5.192102	-0.017797	2.180271
91.416135	1487.673243	5.197107	-0.017870	2.185542
91.714110	1495.763299	5.202112	-0.017931	2.190801
92.159338	1503.848081	5.207117	-0.018019	2.196057
92.601988	1511.892715	5.212122	-0.018107	2.201275
92.845854	1519.966799	5.217126	-0.018158	2.206481
93.534568	1528.023836	5.222131	-0.018291	2.211704
93.838278	1536.118392	5.227136	-0.018353	2.216904
94.046941	1544.218572	5.232141	-0.018397	2.222086
94.642822	1552.264103	5.237146	-0.018514	2.227257
95.162837	1560.349743	5.242150	-0.018616	2.232434
95.300121	1568.461417	5.247155	-0.018647	2.237581
95.516725	1576.522905	5.252160	-0.018692	2.242692
95.742960	1584.621198	5.257165	-0.018740	2.247815
96.088269	1592.707637	5.262170	-0.018809	2.252930
96.482093	1600.759376	5.267174	-0.018888	2.258015
96.947509	1608.813872	5.272179	-0.018980	2.263097
97.278218	1616.887228	5.277184	-0.019047	2.268167
97.594067	1625.059459	5.282189	-0.019111	2.273286
97.946283	1633.096000	5.287194	-0.019182	2.278312
98.125077	1641.163161	5.292198	-0.019220	2.283332
98.543227	1649.220503	5.297203	-0.019303	2.288355
98.937853	1657.273534	5.302208	-0.019382	2.293361
99.328499	1665.335361	5.307213	-0.019460	2.298362
99.604510	1673.409424	5.312218	-0.019517	2.303350
99.508694	1681.532313	5.317222	-0.019504	2.308326
100.054426	1689.598355	5.322227	-0.019611	2.313310
100.252226	1697.654550	5.327232	-0.019653	2.318248
100.368233	1705.729754	5.332237	-0.019680	2.323180
100.634756	1713.790128	5.337242	-0.019735	2.328106
101.291655	1721.837012	5.342246	-0.019863	2.333044
101.531252	1729.925894	5.347251	-0.019913	2.337964
101.478241	1738.017937	5.352256	-0.019908	2.342851
101.664092	1746.108462	5.357261	-0.019948	2.347746
101.930978	1754.201666	5.362266	-0.020003	2.352639
102.126137	1762.250847	5.367270	-0.020045	2.357490
102.589304	1770.277708	5.372275	-0.020136	2.362339
102.793418	1778.333572	5.377280	-0.020180	2.367175
103.334620	1786.387650	5.382285	-0.020286	2.372026
103.898664	1794.416440	5.387290	-0.020396	2.376855
104.271067	1802.471364	5.392294	-0.020470	2.381673
104.352159	1810.578208	5.397299	-0.020491	2.386490
104.721757	1818.637294	5.402304	-0.020565	2.391291
105.348769	1826.688491	5.407309	-0.020687	2.396098
105.572317	1834.764801	5.412314	-0.020734	2.400879
105.825389	1842.815203	5.417318	-0.020786	2.405637
106.280329	1850.883598	5.422323	-0.020876	2.410412
106.604330	1858.966769	5.427328	-0.020942	2.415176
106.682488	1867.058667	5.432333	-0.020962	2.419916
107.082835	1875.093858	5.437338	-0.021042	2.424639
107.337518	1883.166930	5.442342	-0.021094	2.429364
107.798618	1891.314604	5.447347	-0.021186	2.434138
107.683296	1899.378010	5.452352	-0.021169	2.438810
108.300675	1907.355775	5.457357	-0.021290	2.443480
108.348888	1915.438343	5.462362	-0.021304	2.448157
108.623702	1923.504504	5.467366	-0.021360	2.452834
108.884339	1931.562609	5.472371	-0.021414	2.457496
109.101438	1939.591344	5.477376	-0.021460	2.462128
109.271306	1947.667386	5.482381	-0.021497	2.466776
109.638447	1955.736312	5.487386	-0.021570	2.471425
109.950206	1963.782254	5.492390	-0.021634	2.476049
110.327778	1971.812430	5.497395	-0.021709	2.480659
110.506111	1979.857888	5.502400	-0.021748	2.485255
111.006710	1987.908721	5.507405	-0.021846	2.489869
111.315115	1995.982908	5.512410	-0.021909	2.494474
111.406450	2004.052565	5.517414	-0.021931	2.499052
111.685023	2012.124520	5.522419	-0.021988	2.503636
111.974080	2020.174666	5.527424	-0.022048	2.508200
112.043669	2028.304526	5.532429	-0.022066	2.512785
112.254811	2036.353016	5.537434	-0.022110	2.517326
112.517218	2044.356157	5.542438	-0.022165	2.521837
113.005130	2052.399843	5.547443	-0.022261	2.526379
113.311294	2060.438824	5.552448	-0.022323	2.530896
113.556481	2068.535702	5.557453	-0.022374	2.535434
113.897644	2076.558466	5.562458	-0.022443	2.539929
114.152488	2084.589240	5.567462	-0.022495	2.544414
114.547257	2092.672552	5.572467	-0.022574	2.548931
114.500287	2100.765650	5.577472	-0.022571	2.553414
114.805108	2108.802948	5.582477	-0.022633	2.557882
115.202445	2116.841092	5.587482	-0.022712	2.562350
115.341450	2124.891309	5.592486	-0.022743	2.566799
115.679682	2132.952589	5.597491	-0.022811	2.571259
115.959605	2141.018654	5.602496	-0.022869	2.575711
115.945598	2149.095378	5.607501	-0.022872	2.580140
116.181492	2157.128634	5.612506	-0.022921	2.584555
116.273595	2165.203240	5.617510	-0.022943	2.588976
116.616839	2173.408000	5.622515	-0.023012	2.593476
116.902082	2181.425123	5.627520	-0.023071	2.597863
117.181906	2189.414712	5.632525	-0.023128	2.602227
117.427187	2197.423056	5.637530	-0.023179	2.606592
117.738178	2205.456405	5.642534	-0.023242	2.610967
118.182946	2213.517412	5.647539	-0.023330	2.615359
118.116300	2221.554734	5.652544	-0.023323	2.619696
118.523042	2229.589312	5.657549	-0.023404	2.624056
118.795355	2237.629170	5.662554	-0.023460	2.628403
119.125459	2245.688164	5.667558	-0.023527	2.632757
119.248792	2253.751249	5.672563	-0.023555	2.637092
119.386222	2261.776373	5.677568	-0.023586	2.641400
119.570139	2269.839357	5.682573	-0.023626	2.645725
120.150062	2277.841039	5.687578	-0.023739	2.650035
120.408472	2285.897233	5.692582	-0.023792	2.654347
120.518972	2293.981542	5.697587	-0.023818	2.658657
120.699813	2302.017535	5.702592	-0.023857	2.662939
121.173946	2310.030833	5.707597	-0.023951	2.667221
121.334192	2318.120264	5.712602	-0.023986	2.671515
121.559057	2326.190740	5.717606	-0.024033	2.675798
121.920781	2334.209157	5.722611	-0.024106	2.680054
122.152985	2342.218882	5.727616	-0.024154	2.684291
122.500030	2350.261955	5.732621	-0.024224	2.688546
122.543238	2358.361789	5.737626	-0.024237	2.692805
122.737817	2366.406211	5.742630	-0.024279	2.697037
123.150966	2374.436497	5.747635	-0.024361	2.701269
123.625440	2382.445971	5.752640	-0.024455	2.705488
123.782506	2390.500907	5.757645	-0.024489	2.709703
124.149143	2398.593739	5.762650	-0.024563	2.713945
124.389080	2406.620955	5.767654	-0.024613	2.718138
124.895552	2414.634919	5.772659	-0.024712	2.722335
125.103993	2422.671163	5.777664	-0.024756	2.726518
125.543224	2430.719562	5.782669	-0.024843	2.730715
125.957216	2438.782393	5.787674	-0.024926	2.734911
126.043558	2446.830155	5.792678	-0.024947	2.739073
126.328607	2454.880026	5.797683	-0.025005	2.743242
126.569241	2462.921470	5.802688	-0.025055	2.747397
126.751850	2471.032517	5.807693	-0.025095	2.751578
126.920422	2479.153407	5.812698	-0.025131	2.755757
127.226695	2487.127299	5.817702	-0.025194	2.759863
127.611473	2495.130890	5.822707	-0.025271	2.763983
127.742579	2503.166591	5.827712	-0.025300	2.768097
128.197541	2511.203995	5.832717	-0.025390	2.772226
128.295555	2519.259157	5.837722	-0.025414	2.776336
128.307034	2527.307546	5.842726	-0.025421	2.780431
128.838758	2535.303568	5.847731	-0.025526	2.784525
129.136282	2543.348734	5.852736	-0.025586	2.788623
129.358115	2551.424561	5.857741	-0.025633	2.792727
129.513494	2559.493533	5.862746	-0.025667	2.796817
129.888339	2567.509445	5.867750	-0.025742	2.800887
130.122586	2575.534256	5.872755	-0.025791	2.804948
130.241588	2583.573567	5.877760	-0.025818	2.809003
130.489045	2591.656392	5.882765	-0.025870	2.813081
130.711617	2599.712262	5.887770	-0.025916	2.817139
130.999892	2607.734958	5.892774	-0.025975	2.821178
131.507162	2615.730524	5.897779	-0.026075	2.825210
131.860244	2623.766668	5.902784	-0.026146	2.829248
132.235435	2631.870802	5.907789	-0.026221	2.833315
132.707043	2639.886823	5.912794	-0.026314	2.837338
132.850987	2647.918468	5.917798	-0.026346	2.841344
133.052479	2655.944949	5.922803	-0.026389	2.845345
133.247751	2663.986069	5.927808	-0.026431	2.849347
133.647169	2672.024979	5.932813	-0.026510	2.853354
134.123205	2680.078130	5.937818	-0.026604	2.857367
134.215923	2688.115907	5.942822	-0.026627	2.861345
134.509242	2696.153121	5.947827	-0.026687	2.865328
134.729109	2704.184584	5.952832	-0.026733	2.869299
134.920037	2712.269262	5.957837	-0.026774	2.873289
135.004176	2720.336562	5.962842	-0.026795	2.877259
135.442951	2728.316883	5.967846	-0.026882	2.881200
135.589030	2736.367150	5.972851	-0.026914	2.885154
135.615876	2744.415016	5.977856	-0.026925	2.889095
135.890782	2752.484671	5.982861	-0.026981	2.893055
136.253356	2760.511015	5.987866	-0.027054	2.896993
136.326893	2768.549731	5.992870	-0.027073	2.900916
136.645548	2776.571636	5.997875	-0.027137	2.904838
136.836876	2784.624398	6.002880	-0.027178	2.908763
136.798611	2792.764273	6.007885	-0.027176	2.912713
137.216360	2800.805119	6.012890	-0.027260	2.916634
137.400724	2808.789079	6.017894	-0.027299	2.920510
137.491021	2816.795996	6.022899	-0.027321	2.924386
137.582828	2824.801783	6.027904	-0.027343	2.928257
137.822124	2832.866247	6.032909	-0.027393	2.932159
138.178555	2840.903526	6.037914	-0.027465	2.936049
138.265617	2848.899129	6.042918	-0.027486	2.939899
138.647619	2856.928517	6.047923	-0.027563	2.943776
138.848133	2864.976655	6.052928	-0.027605	2.947648
139.223375	2873.025057	6.057933	-0.027681	2.951523
139.609117	2881.071358	6.062938	-0.027758	2.955393
139.856452	2889.065537	6.067942	-0.027809	2.959225
139.953008	2897.121797	6.072947	-0.027832	2.963075
140.170106	2905.165809	6.077952	-0.027878	2.966919
140.415739	2913.216006	6.082957	-0.027929	2.970763
140.735639	2921.282620	6.087962	-0.027994	2.974614
140.767374	2929.314316	6.092966	-0.028005	2.978429
140.726749	2937.361413	6.097971	-0.028003	2.982242
140.918718	2945.376881	6.102976	-0.028044	2.986047
141.043068	2953.426382	6.107981	-0.028072	2.989860
141.253594	2961.514133	6.112986	-0.028117	2.993690
141.572624	2969.496230	6.117990	-0.028181	2.997471
141.834694	2977.539693	6.122995	-0.028235	3.001274
141.969928	2985.525873	6.128000	-0.028266	3.005038
142.267444	2993.565557	6.133005	-0.028326	3.008830
142.594408	3001.635086	6.138010	-0.028393	3.012634
142.726094	3009.688153	6.143014	-0.028422	3.016415
142.927083	3017.708775	6.148019	-0.028465	3.020179
143.079346	3025.702514	6.153024	-0.028499	3.023924
143.290219	3033.762352	6.158029	-0.028543	3.027698
143.724897	3041.805713	6.163034	-0.028629	3.031470
144.003976	3049.835925	6.168038	-0.028687	3.035224
144.211093	3057.857507	6.173043	-0.028730	3.038966
144.432139	3065.903783	6.178048	-0.028777	3.042715
144.535660	3073.931186	6.183053	-0.028801	3.046445
145.106397	3081.933781	6.188058	-0.028913	3.050182
145.270968	3090.003824	6.193062	-0.028949	3.053925
145.485934	3098.050981	6.198067	-0.028994	3.057656
145.670461	3106.070617	6.203072	-0.029034	3.061368
145.903966	3114.097784	6.208077	-0.029083	3.065081
145.947750	3122.167759	6.213082	-0.029096	3.068801
146.189128	3130.247096	6.218086	-0.029146	3.072530
146.482126	3138.320250	6.223091	-0.029206	3.076253
146.591702	3146.283128	6.228096	-0.029232	3.079913
146.893496	3154.290568	6.233101	-0.029293	3.083598
147.178785	3162.316921	6.238106	-0.029352	3.087286
147.283194	3170.363780	6.243110	-0.029376	3.090971
147.718441	3178.375328	6.248115	-0.029463	3.094651
147.830008	3186.390861	6.253120	-0.029489	3.098313
148.033208	3194.453355	6.258125	-0.029532	3.101996
148.418700	3202.462663	6.263130	-0.029609	3.105659
148.497699	3210.508850	6.268134	-0.029629	3.109321
148.741197	3218.577729	6.273139	-0.029679	3.112996
148.916834	3226.622398	6.278144	-0.029717	3.116652
149.126030	3234.603626	6.283149	-0.029762	3.120277
149.710274	3242.598451	6.288154	-0.029876	3.123921
149.814481	3250.665664	6.293158	-0.029900	3.127571
149.870242	3258.738156	6.298163	-0.029916	3.131218
150.189277	3266.756015	6.303168	-0.029981	3.134847
150.353531	3274.800654	6.308173	-0.030016	3.138477
150.697111	3282.793327	6.313178	-0.030086	3.142088
150.956073	3290.818967	6.318182	-0.030139	3.145706
151.089981	3298.869702	6.323187	-0.030169	3.149325
151.136823	3306.941761	6.328192	-0.030183	3.152945
151.454597	3314.953464	6.333197	-0.030248	3.156546
151.786961	3322.969570	6.338202	-0.030315	3.160146
151.764228	3331.005694	6.343206	-0.030316	3.163735
152.113279	3339.021914	6.348211	-0.030386	3.167327
151.983118	3347.051006	6.353216	-0.030367	3.170900
152.345826	3355.121517	6.358221	-0.030440	3.174509
152.647100	3363.150419	6.363226	-0.030501	3.178093
152.674824	3371.186705	6.368230	-0.030512	3.181664
152.994516	3379.200514	6.373235	-0.030577	3.185233
153.364199	3387.213053	6.378240	-0.030651	3.188800
153.497807	3395.270715	6.383245	-0.030681	3.192373
153.700969	3403.329433	6.388250	-0.030724	3.195945
153.982920	3411.295016	6.393254	-0.030782	3.199475
154.218896	3419.334794	6.398259	-0.030831	3.203032
154.362901	3427.378881	6.403264	-0.030863	3.206584
154.568152	3435.431850	6.408269	-0.030907	3.210137
154.622534	3443.486778	6.413274	-0.030922	3.213682
154.724597	3451.507742	6.418278	-0.030946	3.217209
155.032639	3459.530311	6.423283	-0.031009	3.220742
155.208994	3467.530724	6.428288	-0.031047	3.224256
155.278798	3475.562058	6.433293	-0.031065	3.227775
155.692046	3483.635121	6.438298	-0.031147	3.231323
155.710097	3491.706906	6.443302	-0.031156	3.234850
156.102384	3499.701887	6.448307	-0.031234	3.238354
156.131035	3507.709380	6.453312	-0.031245	3.241846
156.421387	3515.681202	6.458317	-0.031304	3.245329
156.801936	3523.721626	6.463322	-0.031380	3.248842
156.839782	3531.747911	6.468326	-0.031393	3.252330
156.933626	3539.841742	6.473331	-0.031415	3.255847
157.097382	3547.815472	6.478336	-0.031451	3.259311
157.356079	3555.834510	6.483341	-0.031505	3.262794
157.706975	3563.877646	6.488346	-0.031575	3.266287
157.809669	3571.898009	6.493350	-0.031600	3.269757
157.972230	3579.996027	6.498355	-0.031635	3.273260
158.089325	3588.037398	6.503360	-0.031662	3.276732
158.375216	3596.003896	6.508365	-0.031721	3.280175
158.621982	3604.026002	6.513370	-0.031772	3.283637
158.555697	3612.046449	6.518374	-0.031765	3.287082
158.934896	3620.105715	6.523379	-0.031841	3.290557
159.268653	3628.139184	6.528384	-0.031908	3.294016
159.293758	3636.179060	6.533389	-0.031918	3.297462
159.560919	3644.204973	6.538394	-0.031973	3.300908
159.735838	3652.166561	6.543398	-0.032011	3.304319
160.069016	3660.215966	6.548403	-0.032078	3.307770
160.192826	3668.326234	6.553408	-0.032107	3.311235
160.451223	3676.326137	6.558413	-0.032160	3.314655
160.911893	3684.338534	6.563418	-0.032251	3.318084
160.926986	3692.345934	6.568422	-0.032259	3.321491
161.140826	3700.355080	6.573427	-0.032304	3.324903
161.423645	3708.372381	6.578432	-0.032362	3.328316
161.673513	3716.439988	6.583437	-0.032414	3.331747
161.730067	3724.491669	6.588442	-0.032430	3.335160
161.896605	3732.505118	6.593446	-0.032466	3.338557
162.238311	3740.524111	6.598451	-0.032535	3.341960
162.263260	3748.541272	6.603456	-0.032545	3.345347
162.622959	3756.561963	6.608461	-0.032617	3.348744
162.756913	3764.648319	6.613466	-0.032647	3.352157
162.755336	3772.691633	6.618470	-0.032652	3.355543
163.185734	3780.673916	6.623475	-0.032738	3.358916
163.268806	3788.698019	6.628480	-0.032758	3.362291
163.437585	3796.714690	6.633485	-0.032795	3.365662
163.474121	3804.767193	6.638490	-0.032807	3.369040
163.598697	3812.808354	6.643494	-0.032836	3.372413
164.169474	3820.829313	6.648499	-0.032947	3.375790
164.137057	3828.844116	6.653504	-0.032946	3.379140
164.228674	3836.892988	6.658509	-0.032969	3.382504
164.536291	3844.906192	6.663514	-0.033031	3.385859
164.740887	3852.906968	6.668518	-0.033074	3.389201
164.699494	3861.049736	6.673523	-0.033072	3.392590
165.064301	3869.096664	6.678528	-0.033145	3.395950
165.244953	3877.025880	6.683533	-0.033184	3.399252
165.508987	3885.043192	6.688538	-0.033239	3.402590
165.405629	3893.060764	6.693542	-0.033225	3.405911
165.995772	3901.057775	6.698547	-0.033340	3.409245
166.166241	3909.108326	6.703552	-0.033377	3.412584
166.427087	3917.138209	6.708557	-0.033431	3.415913
166.914360	3925.136167	6.713562	-0.033527	3.419234
166.923532	3933.180814	6.718566	-0.033534	3.422555
167.135876	3941.205962	6.723571	-0.033578	3.425871
167.308158	3949.236215	6.728576	-0.033616	3.429185
167.453847	3957.289404	6.733581	-0.033648	3.432504
167.644844	3965.350560	6.738586	-0.033689	3.435824
167.934896	3973.337009	6.743590	-0.033748	3.439114
168.281213	3981.341137	6.748595	-0.033818	3.442410
168.445782	3989.351847	6.753600	-0.033854	3.445699
168.457369	3997.380387	6.758605	-0.033861	3.448988
168.746590	4005.473584	6.763610	-0.033920	3.452309
168.711232	4013.493875	6.768614	-0.033919	3.455586
168.943528	4021.507151	6.773619	-0.033968	3.458866
169.236731	4029.514079	6.778624	-0.034027	3.462142
169.544056	4037.490821	6.783629	-0.034090	3.465403
169.667962	4045.581137	6.788634	-0.034118	3.468702
170.025915	4053.591496	6.793638	-0.034190	3.471972
170.376270	4061.647073	6.798643	-0.034261	3.475257
170.505237	4069.672584	6.803648	-0.034290	3.478520
170.523569	4077.679016	6.808653	-0.034299	3.481769
170.933788	4085.674397	6.813658	-0.034380	3.485022
170.955504	4093.709521	6.818662	-0.034390	3.488276
171.131604	4101.764000	6.823667	-0.034428	3.491540
171.251090	4109.777202	6.828672	-0.034455	3.494782
171.359144	4117.793384	6.833677	-0.034480	3.498022
171.580025	4125.849315	6.838682	-0.034527	3.501279
171.702817	4133.786388	6.843686	-0.034555	3.504481
172.250405	4141.838306	6.848691	-0.034662	3.507740
172.404410	4149.895756	6.853696	-0.034696	3.510986
172.439676	4157.929473	6.858701	-0.034708	3.514216
172.632038	4165.956199	6.863706	-0.034749	3.517445
172.739685	4173.961071	6.868710	-0.034774	3.520659
173.049851	4181.957054	6.873715	-0.034837	3.523873
173.181331	4189.986593	6.878720	-0.034867	3.527092
173.461038	4198.043492	6.883725	-0.034924	3.530324
173.799977	4206.097165	6.888730	-0.034993	3.533553
173.725554	4214.118463	6.893734	-0.034984	3.536754
173.933605	4222.135076	6.898739	-0.035028	3.539958
174.075917	4230.164788	6.903744	-0.035060	3.543163
174.325691	4238.188282	6.908749	-0.035112	3.546365
174.438362	4246.247475	6.913754	-0.035138	3.549575
174.481346	4254.321584	6.918758	-0.035151	3.552786
174.850930	4262.392064	6.923763	-0.035225	3.556002
175.169600	4270.312430	6.928768	-0.035290	3.559154
175.288024	4278.299720	6.933773	-0.035317	3.562323
175.447715	4286.319524	6.938778	-0.035352	3.565504
175.497773	4294.333341	6.943782	-0.035367	3.568677
175.917275	4302.382457	6.948787	-0.035450	3.571871
176.033066	4310.418548	6.953792	-0.035477	3.575049
176.261528	4318.430657	6.958797	-0.035525	3.578218
176.490272	4326.459463	6.963802	-0.035573	3.581390
176.581190	4334.419897	6.968806	-0.035595	3.584528
176.881905	4342.488787	6.973811	-0.035656	3.587713
176.694419	4350.548687	6.978816	-0.035627	3.590877
177.112315	4358.551264	6.983821	-0.035710	3.594033
177.368286	4366.589433	6.988826	-0.035763	3.597196
177.514129	4374.568641	6.993830	-0.035795	3.600329
177.748039	4382.577264	6.998835	-0.035844	3.603474
177.897534	4390.613381	7.003840	-0.035877	3.606624
177.875800	4398.633657	7.008845	-0.035878	3.609761
178.116948	4406.703779	7.013850	-0.035928	3.612922
178.281605	4414.708112	7.018854	-0.035964	3.616052
178.600229	4422.705388	7.023859	-0.036029	3.619181
178.599589	4430.757856	7.028864	-0.036034	3.622320
178.741185	4438.764022	7.033869	-0.036065	3.625442
178.966040	4446.829924	7.038874	-0.036113	3.628586
179.139031	4454.855942	7.043878	-0.036150	3.631711
179.511213	4462.899209	7.048883	-0.036225	3.634846
179.459732	4470.933946	7.053888	-0.036220	3.637963
179.532319	4478.914614	7.058893	-0.036239	3.641060
179.894238	4486.907127	7.063898	-0.036312	3.644166
180.060354	4494.906395	7.068902	-0.036348	3.647267
180.159026	4502.960788	7.073907	-0.036372	3.650385
180.475795	4511.016078	7.078912	-0.036436	3.653506
180.843736	4519.036086	7.083917	-0.036510	3.656613
180.933748	4527.056907	7.088922	-0.036532	3.659710
180.905457	4535.075584	7.093926	-0.036532	3.662800
181.045422	4543.128565	7.098931	-0.036563	3.665905
181.175755	4551.115233	7.103936	-0.036592	3.668982
181.390370	4559.172859	7.108941	-0.036638	3.672085
181.661878	4567.169358	7.113946	-0.036694	3.675164
181.876553	4575.187072	7.118950	-0.036739	3.678247
182.010484	4583.246320	7.123955	-0.036769	3.681341
182.221698	4591.189902	7.128960	-0.036814	3.684391
182.313102	4599.262319	7.133965	-0.036836	3.687484
182.457760	4607.295584	7.138970	-0.036868	3.690560
182.563752	4615.316929	7.143974	-0.036893	3.693629
183.054612	4623.337689	7.148979	-0.036990	3.696704
183.323554	4631.322603	7.153984	-0.037045	3.699758
183.383105	4639.363969	7.158989	-0.037061	3.702825
183.529579	4647.394894	7.163994	-0.037094	3.705888
183.741620	4655.397916	7.168998	-0.037139	3.708940
183.989296	4663.485804	7.174003	-0.037190	3.712022
183.868197	4671.582972	7.179008	-0.037173	3.715096
184.353182	4679.504650	7.184013	-0.037268	3.718115
185.519115	4687.489728	7.189018	-0.037491	3.721173
185.593648	4695.442139	7.194022	-0.037510	3.724189
186.044852	4703.498233	7.199027	-0.037599	3.727251
186.138108	4711.520370	7.204032	-0.037622	3.730289
186.345237	4719.560875	7.209037	-0.037665	3.733335
186.781534	4727.635722	7.214042	-0.037752	3.736396
186.722016	4735.601357	7.219046	-0.037746	3.739401
187.028668	4743.650575	7.224051	-0.037809	3.742445
187.241526	4751.626173	7.229056	-0.037853	3.745455
187.396663	4759.685708	7.234061	-0.037888	3.748494
187.536770	4767.769396	7.239066	-0.037919	3.751539
187.532031	4775.761539	7.244070	-0.037923	3.754544
188.134678	4783.779066	7.249075	-0.038041	3.757569
188.172089	4791.794901	7.254080	-0.038053	3.760579
188.122709	4799.790870	7.259085	-0.038049	3.763577
188.493490	4807.867474	7.264090	-0.038123	3.766612
188.657665	4815.859949	7.269094	-0.038159	3.769608
188.829236	4823.928533	7.274099	-0.038196	3.772631
188.951161	4831.959898	7.279104	-0.038224	3.775636
188.818595	4839.938700	7.284109	-0.038205	3.778614
189.051748	4848.002946	7.289114	-0.038254	3.781629
189.201419	4855.984962	7.294118	-0.038287	3.784609
189.536723	4864.006642	7.299123	-0.038354	3.787606
189.739797	4872.034336	7.304128	-0.038398	3.790600
189.780153	4880.080672	7.309133	-0.038410	3.793594
190.017842	4888.166214	7.314138	-0.038460	3.796606
189.989661	4896.067172	7.319142	-0.038460	3.799540
190.039549	4904.118564	7.324147	-0.038474	3.802530
190.224711	4912.110273	7.329152	-0.038514	3.805498
190.352555	4920.123463	7.334157	-0.038543	3.808470
190.575480	4928.182973	7.339162	-0.038590	3.811460
190.602259	4936.193637	7.344166	-0.038600	3.814424
190.950179	4944.192788	7.349171	-0.038670	3.817389
191.257695	4952.223475	7.354176	-0.038733	3.820363
191.352210	4960.189059	7.359181	-0.038756	3.823305
191.500200	4968.277147	7.364186	-0.038788	3.826292
191.675167	4976.270092	7.369190	-0.038826	3.829241
192.106141	4984.331022	7.374195	-0.038912	3.832219
192.210506	4992.326998	7.379200	-0.038936	3.835164
192.239527	5000.314748	7.384205	-0.038947	3.838101
192.473435	5008.383786	7.389210	-0.038996	3.841071
192.764063	5016.336895	7.394214	-0.039055	3.843997
192.753856	5024.416905	7.399219	-0.039059	3.846961
193.033777	5032.405168	7.404224	-0.039116	3.849895
192.995522	5040.489822	7.409229	-0.039114	3.852856
193.260774	5048.540827	7.414234	-0.039169	3.855808
193.471554	5056.503781	7.419238	-0.039213	3.858724
193.646919	5064.547447	7.424243	-0.039251	3.861668
193.721311	5072.540436	7.429248	-0.039270	3.864588
193.827720	5080.595962	7.434253	-0.039295	3.867529
194.246106	5088.638120	7.439258	-0.039379	3.870470
194.853988	5096.795461	7.444262	-0.039497	3.873454
195.252321	5104.833425	7.449267	-0.039577	3.876388
195.500285	5112.730357	7.454272	-0.039628	3.879266
195.597513	5120.725554	7.459277	-0.039651	3.882174
195.945737	5128.742610	7.464282	-0.039721	3.885093
196.146063	5136.758242	7.469286	-0.039764	3.888006
196.316466	5144.748843	7.474291	-0.039801	3.890907
196.501492	5152.798146	7.479296	-0.039841	3.893828
196.422745	5160.853677	7.484301	-0.039831	3.896743
196.946657	5168.802451	7.489306	-0.039934	3.899630
196.987303	5176.814575	7.494310	-0.039947	3.902527
196.936230	5184.845237	7.499315	-0.039943	3.905428
197.096801	5192.882980	7.504320	-0.039978	3.908333
197.156825	5200.882636	7.509325	-0.039994	3.911220
197.481930	5208.962943	7.514330	-0.040060	3.914139
197.530825	5216.953500	7.519334	-0.040074	3.917019
197.876390	5224.933061	7.524339	-0.040144	3.919898
197.955574	5232.945234	7.529344	-0.040164	3.922781
197.992820	5240.970684	7.534349	-0.040176	3.925666
198.261586	5248.998186	7.539354	-0.040231	3.928555
198.495524	5257.017807	7.544358	-0.040280	3.931437
198.724903	5265.041038	7.549363	-0.040328	3.934319
198.819346	5273.076126	7.554368	-0.040351	3.937200
199.222129	5281.073895	7.559373	-0.040431	3.940071
199.354190	5289.105933	7.564378	-0.040461	3.942948
199.108140	5297.124141	7.569382	-0.040421	3.945811
199.634489	5305.132812	7.574387	-0.040524	3.948682
199.642706	5313.177298	7.579392	-0.040531	3.951554
199.631234	5321.199723	7.584397	-0.040534	3.954417
199.986260	5329.226795	7.589402	-0.040605	3.957285
200.270767	5337.192260	7.594406	-0.040663	3.960128
200.651484	5345.237010	7.599411	-0.040740	3.962998
200.584657	5353.239899	7.604416	-0.040732	3.965844
200.500671	5361.246701	7.609421	-0.040722	3.968690
200.813634	5369.322954	7.614426	-0.040786	3.971564
200.896058	5377.314959	7.619430	-0.040806	3.974402
201.134409	5385.372265	7.624435	-0.040856	3.977265
201.329041	5393.352960	7.629440	-0.040897	3.980097
201.514349	5401.377778	7.634445	-0.040937	3.982943
201.764673	5409.378919	7.639450	-0.040989	3.985779
201.831407	5417.392635	7.644454	-0.041007	3.988615
201.844232	5425.460528	7.649459	-0.041014	3.991467
202.230921	5433.505488	7.654464	-0.041092	3.994315
202.622659	5441.530469	7.659469	-0.041170	3.997153
202.756140	5449.508484	7.664474	-0.041200	3.999969
202.772462	5457.524096	7.669478	-0.041208	4.002795
202.912238	5465.548662	7.674483	-0.041239	4.005623
203.295891	5473.555546	7.679488	-0.041316	4.008448
203.383581	5481.566438	7.684493	-0.041338	4.011266
203.364279	5489.677543	7.689498	-0.041339	4.014117
203.701160	5497.686967	7.694502	-0.041407	4.016935
203.929953	5505.679368	7.699507	-0.041455	4.019744
203.952577	5513.713273	7.704512	-0.041465	4.022562
204.400772	5521.674429	7.709517	-0.041553	4.025359
204.711662	5529.732932	7.714522	-0.041617	4.028186
204.731558	5537.734048	7.719526	-0.041626	4.030986
204.973854	5545.854342	7.724531	-0.041676	4.033829
205.038652	5553.886257	7.729536	-0.041693	4.036637
205.007872	5561.784820	7.734541	-0.041693	4.039395
205.372694	5569.865158	7.739546	-0.041766	4.042221
205.538234	5577.774418	7.744550	-0.041802	4.044982
205.608058	5585.825840	7.749555	-0.041820	4.047789
205.664765	5593.841294	7.754560	-0.041836	4.050581
205.926399	5601.870757	7.759565	-0.041890	4.053379
206.200077	5609.932324	7.764570	-0.041946	4.056187
206.173330	5617.898864	7.769574	-0.041947	4.058955
206.368172	5625.928210	7.774579	-0.041988	4.061746
206.628674	5633.944266	7.779584	-0.042042	4.064532
206.679873	5641.946605	7.784589	-0.042057	4.067308
206.904337	5649.978006	7.789594	-0.042104	4.070095
207.112411	5658.003054	7.794598	-0.042148	4.072877
207.334403	5666.041243	7.799603	-0.042194	4.075662
207.555004	5674.020072	7.804608	-0.042241	4.078425
207.890467	5682.018787	7.809613	-0.042308	4.081194
208.013885	5690.061368	7.814618	-0.042337	4.083974
208.190961	5698.072976	7.819622	-0.042375	4.086742
208.245832	5706.100349	7.824627	-0.042390	4.089511
208.383430	5714.167096	7.829632	-0.042421	4.092293
208.562082	5722.162540	7.834637	-0.042460	4.095050
208.785117	5730.190760	7.839642	-0.042507	4.097816
208.724659	5738.181901	7.844646	-0.042500	4.100564
208.897193	5746.181231	7.849651	-0.042538	4.103316
209.317415	5754.222896	7.854656	-0.042621	4.106084
209.397496	5762.229447	7.859661	-0.042642	4.108834
209.664004	5770.340853	7.864666	-0.042696	4.111620
209.891004	5778.325451	7.869670	-0.042744	4.114360
209.812367	5786.367956	7.874675	-0.042735	4.117114
210.070325	5794.324815	7.879680	-0.042788	4.119842
210.298556	5802.331979	7.884685	-0.042836	4.122584
210.507524	5810.367210	7.889690	-0.042880	4.125334
210.506694	5818.391835	7.894694	-0.042885	4.128076
210.744225	5826.376509	7.899699	-0.042934	4.130805
210.992606	5834.479669	7.904704	-0.042986	4.133573
211.049145	5842.490892	7.909709	-0.043002	4.136305
211.249393	5850.491280	7.914714	-0.043044	4.139034
211.450892	5858.478650	7.919718	-0.043087	4.141756
211.608724	5866.486684	7.924723	-0.043122	4.144483
211.741796	5874.585427	7.929728	-0.043152	4.147239
211.900084	5882.575702	7.934733	-0.043186	4.149956
212.293843	5890.618227	7.939738	-0.043265	4.152693
212.352428	5898.613469	7.944742	-0.043281	4.155407
212.532479	5906.613453	7.949747	-0.043320	4.158122
212.536645	5914.647830	7.954752	-0.043326	4.160846
212.615535	5922.620387	7.959757	-0.043346	4.163547
213.101661	5930.695028	7.964762	-0.043442	4.166286
213.014236	5938.669945	7.969766	-0.043431	4.168983
212.847170	5946.726576	7.974771	-0.043405	4.171705
213.141678	5954.735086	7.979776	-0.043465	4.174414
213.281498	5962.784590	7.984781	-0.043496	4.177133
213.548556	5970.753750	7.989786	-0.043551	4.179825
213.463537	5978.797145	7.994790	-0.043541	4.182536
213.787700	5986.746186	7.999795	-0.043606	4.185218
214.040870	5994.851156	8.004800	-0.043659	4.187950
214.200572	6002.818843	8.009805	-0.043694	4.190633
214.651596	6010.937455	8.014810	-0.043783	4.193368
214.781309	6018.963074	8.019814	-0.043812	4.196067
215.067750	6026.903413	8.024819	-0.043871	4.198737
215.200268	6034.890991	8.029824	-0.043901	4.201419
215.516103	6042.831451	8.034829	-0.043965	4.204086
215.705840	6050.945907	8.039834	-0.044005	4.206808
215.824537	6058.907552	8.044838	-0.044033	4.209476
216.087566	6066.972488	8.049843	-0.044087	4.212179
215.999016	6074.999299	8.054848	-0.044076	4.214864
216.178142	6082.986662	8.059853	-0.044114	4.217536
216.361730	6090.993992	8.064858	-0.044154	4.220214
216.542336	6099.007514	8.069862	-0.044193	4.222891
216.760869	6107.000744	8.074867	-0.044239	4.225561
216.976633	6115.036665	8.079872	-0.044284	4.228243
217.184621	6123.033972	8.084877	-0.044328	4.230911
217.249051	6131.110921	8.089882	-0.044345	4.233601
217.427621	6139.137200	8.094886	-0.044384	4.236275
217.696718	6147.100310	8.099891	-0.044439	4.238926
217.827169	6155.176756	8.104896	-0.044469	4.241613
217.938197	6163.106651	8.109901	-0.044495	4.244248
218.189792	6171.182422	8.114906	-0.044547	4.246932
218.434615	6179.149715	8.119910	-0.044598	4.249578
218.569773	6187.228723	8.124915	-0.044628	4.252258
218.850440	6195.276839	8.129920	-0.044686	4.254928
218.918448	6203.259569	8.134925	-0.044704	4.257572
218.862921	6211.297834	8.139930	-0.044698	4.260232
219.025432	6219.316341	8.144934	-0.044734	4.262886
219.361049	6227.301269	8.149939	-0.044802	4.265528
219.432840	6235.363538	8.154944	-0.044820	4.268192
219.380005	6243.343360	8.159949	-0.044816	4.270826
219.580552	6251.468167	8.164954	-0.044858	4.273508
219.708037	6259.471259	8.169958	-0.044887	4.276148
219.958665	6267.419313	8.174963	-0.044939	4.278770
220.091415	6275.437959	8.179968	-0.044969	4.281412
220.438973	6283.386887	8.184973	-0.045039	4.284031
220.366630	6291.498591	8.189978	-0.045031	4.286698
220.332184	6299.464267	8.194982	-0.045030	4.289316
220.544205	6307.521844	8.199987	-0.045075	4.291965
220.815357	6315.564009	8.204992	-0.045130	4.294607
221.040600	6323.571439	8.209997	-0.045178	4.297236
221.331249	6331.514662	8.215002	-0.045237	4.299843
221.589567	6339.600842	8.220006	-0.045290	4.302495
221.677652	6347.596057	8.225011	-0.045312	4.305114
221.742697	6355.632035	8.230016	-0.045329	4.307745
221.880279	6363.594874	8.235021	-0.045360	4.310350
221.956727	6371.711142	8.240026	-0.045380	4.313004
222.039031	6379.688921	8.245030	-0.045400	4.315611
222.257524	6387.671315	8.250035	-0.045446	4.318219
222.609941	6395.676646	8.255040	-0.045517	4.320833
222.631703	6403.676221	8.260045	-0.045526	4.323442
222.780993	6411.729545	8.265050	-0.045559	4.326068
222.890392	6419.758029	8.270054	-0.045585	4.328683
222.919429	6427.774953	8.275059	-0.045596	4.331293
223.252809	6435.815079	8.280064	-0.045663	4.333911
223.383820	6443.821338	8.285069	-0.045693	4.336515
223.773735	6451.839441	8.290074	-0.045771	4.339122
223.455417	6459.861156	8.295078	-0.045717	4.341725
223.648364	6467.814300	8.300083	-0.045758	4.344307
223.966682	6475.868840	8.305088	-0.045822	4.346921
223.865544	6483.861835	8.310093	-0.045809	4.349511
224.124089	6491.920686	8.315098	-0.045862	4.352124
224.191970	6500.014383	8.320102	-0.045880	4.354744
224.383778	6508.023642	8.325107	-0.045921	4.357337
224.469535	6515.935543	8.330112	-0.045942	4.359896
224.807268	6523.937073	8.335117	-0.046010	4.362483
225.134876	6531.949496	8.340122	-0.046077	4.365073
225.207561	6539.995899	8.345126	-0.046095	4.367671
225.346355	6547.986815	8.350131	-0.046126	4.370249
225.668637	6556.061405	8.355136	-0.046192	4.372854
225.526348	6564.052663	8.360141	-0.046171	4.375428
225.917747	6572.058144	8.365146	-0.046249	4.378008
226.251956	6580.033647	8.370150	-0.046316	4.380576
226.150768	6588.063577	8.375155	-0.046303	4.383158
226.175862	6596.076524	8.380160	-0.046312	4.385734
226.522529	6604.077832	8.385165	-0.046382	4.388306
226.804012	6612.147375	8.390170	-0.046440	4.390898
226.668233	6620.194938	8.395174	-0.046420	4.393480
226.724900	6628.206896	8.400179	-0.046436	4.396049
227.275311	6636.208426	8.405184	-0.046543	4.398616
227.336754	6644.218131	8.410189	-0.046560	4.401182
227.556044	6652.212381	8.415194	-0.046606	4.403742
227.693605	6660.263471	8.420198	-0.046637	4.406318
228.056107	6668.231715	8.425203	-0.046710	4.408868
228.039663	6676.293818	8.430208	-0.046712	4.411444
227.969206	6684.278358	8.435213	-0.046704	4.413993
228.287525	6692.370082	8.440218	-0.046769	4.416577
228.328929	6700.341679	8.445222	-0.046782	4.419120
228.644139	6708.378412	8.450227	-0.046846	4.421683
228.901521	6716.327684	8.455232	-0.046899	4.424217
228.735597	6724.380047	8.460237	-0.046873	4.426780
228.917674	6732.407429	8.465242	-0.046912	4.429336
229.079204	6740.496775	8.470246	-0.046948	4.431909
229.219799	6748.496870	8.475251	-0.046979	4.434453
229.349092	6756.545034	8.480256	-0.047009	4.437010
229.491602	6764.469846	8.485261	-0.047040	4.439527
229.920612	6772.538046	8.490266	-0.047125	4.442089
230.051584	6780.458483	8.495270	-0.047155	4.444601
230.171263	6788.536336	8.500275	-0.047183	4.447161
230.337788	6796.538434	8.505280	-0.047219	4.449697
230.431631	6804.587530	8.510285	-0.047242	4.452245
230.544310	6812.599590	8.515290	-0.047268	4.454781
230.610898	6820.628689	8.520294	-0.047286	4.457320
230.946022	6828.589955	8.525299	-0.047353	4.459837
231.117846	6836.687343	8.530304	-0.047390	4.462395
231.034874	6844.602512	8.535309	-0.047380	4.464893
231.420789	6852.677996	8.540314	-0.047457	4.467443
231.558894	6860.670950	8.545318	-0.047488	4.469963
231.646296	6868.696796	8.550323	-0.047510	4.472493
231.733565	6876.767882	8.555328	-0.047531	4.475035
231.933508	6884.728286	8.560333	-0.047574	4.477541
232.026117	6892.718202	8.565338	-0.047596	4.480055
232.136311	6900.759150	8.570343	-0.047622	4.482584
232.363738	6908.733920	8.575347	-0.047670	4.485090
232.492966	6916.815663	8.580352	-0.047699	4.487629
232.645002	6924.780433	8.585357	-0.047733	4.490129
233.149937	6932.825943	8.590362	-0.047832	4.492655
233.024896	6940.859237	8.595367	-0.047814	4.495173
233.096487	6948.866271	8.600371	-0.047832	4.497682
233.699587	6956.873987	8.605376	-0.047950	4.500191
233.864795	6964.878332	8.610381	-0.047986	4.502697
234.014659	6972.917292	8.615386	-0.048019	4.505212
233.940287	6980.942736	8.620391	-0.048011	4.507721
234.121925	6988.908541	8.625395	-0.048050	4.510211
234.339842	6997.025533	8.630400	-0.048096	4.512746
234.477885	7004.998731	8.635405	-0.048126	4.515235
234.603031	7013.056578	8.640410	-0.048155	4.517749
234.894778	7020.985498	8.645415	-0.048215	4.520221
235.148903	7028.967262	8.650419	-0.048267	4.522709
235.079665	7037.007978	8.655424	-0.048259	4.525213
235.177656	7044.994778	8.660429	-0.048283	4.527699
235.423526	7053.037221	8.665434	-0.048334	4.530201
235.725964	7061.077818	8.670439	-0.048396	4.532702
235.751304	7069.080519	8.675443	-0.048406	4.535188
236.039683	7077.096068	8.680448	-0.048465	4.537678
236.018927	7085.094840	8.685453	-0.048466	4.540161
236.364697	7093.143193	8.690458	-0.048536	4.542658
236.428506	7101.113078	8.695463	-0.048553	4.545129
236.356732	7109.174733	8.700467	-0.048545	4.547627
236.540557	7117.189059	8.705472	-0.048584	4.550109
236.750211	7125.211748	8.710477	-0.048628	4.552593
236.961309	7133.293413	8.715482	-0.048673	4.555093
236.974918	7141.279512	8.720487	-0.048681	4.557562
237.300632	7149.196832	8.725491	-0.048747	4.560009
237.312077	7157.262429	8.730496	-0.048754	4.562500
237.357651	7165.225072	8.735501	-0.048768	4.564958
237.428046	7173.304295	8.740506	-0.048786	4.567451
237.533256	7181.294664	8.745511	-0.048811	4.569915
237.724462	7189.355979	8.750515	-0.048852	4.572399
237.985724	7197.371856	8.755520	-0.048906	4.574869
238.013371	7205.381723	8.760525	-0.048916	4.577334
238.233085	7213.366961	8.765530	-0.048962	4.579791
238.367998	7221.418755	8.770535	-0.048993	4.582267
238.501700	7229.382502	8.775539	-0.049023	4.584715
238.394067	7237.494457	8.780544	-0.049008	4.587207
238.513142	7245.423155	8.785549	-0.049035	4.589641
238.765051	7253.528886	8.790554	-0.049088	4.592128
239.052729	7261.557594	8.795559	-0.049147	4.594591
239.114481	7269.561515	8.800563	-0.049163	4.597044
239.453765	7277.493953	8.805568	-0.049232	4.599474
239.458674	7285.533083	8.810573	-0.049238	4.601935
239.759283	7293.482378	8.815578	-0.049299	4.604368
239.800053	7301.567897	8.820583	-0.049312	4.606841
239.879247	7309.520872	8.825587	-0.049332	4.609272
240.265915	7317.673218	8.830592	-0.049409	4.611763
240.305790	7325.617448	8.835597	-0.049422	4.614189
240.479002	7333.677426	8.840602	-0.049459	4.616648
240.816980	7341.601564	8.845607	-0.049527	4.619065
240.751240	7349.660917	8.850611	-0.049521	4.621522
241.087611	7357.684837	8.855616	-0.049588	4.623967
241.146385	7365.693421	8.860621	-0.049605	4.626406
241.382619	7373.681825	8.865626	-0.049654	4.628838
241.221668	7381.735625	8.870631	-0.049629	4.631288
241.294418	7389.710780	8.875635	-0.049648	4.633713
241.740574	7397.813045	8.880640	-0.049736	4.636175
241.556331	7405.732547	8.885645	-0.049707	4.638580
241.785823	7413.783463	8.890650	-0.049755	4.641024
242.143196	7421.764899	8.895655	-0.049827	4.643446
242.167246	7429.799272	8.900659	-0.049837	4.645882
242.284682	7437.814426	8.905664	-0.049864	4.648311
242.553021	7445.821879	8.910669	-0.049919	4.650737
242.666817	7453.881637	8.915674	-0.049946	4.653177
242.672358	7461.912309	8.920679	-0.049952	4.655607
242.960862	7469.906847	8.925683	-0.050011	4.658025
243.167761	7477.938422	8.930688	-0.050055	4.660452
243.177223	7485.911512	8.935693	-0.050062	4.662861
243.191222	7493.913574	8.940698	-0.050069	4.665278
243.431371	7501.943502	8.945703	-0.050119	4.667701
243.317085	7509.913012	8.950707	-0.050103	4.670105
243.710855	7518.042196	8.955712	-0.050182	4.672556
243.612297	7526.091601	8.960717	-0.050169	4.674981
244.056837	7534.086672	8.965722	-0.050257	4.677389
244.021644	7541.996436	8.970727	-0.050256	4.679770
244.083492	7550.017643	8.975731	-0.050272	4.682183
244.433011	7558.012420	8.980736	-0.050343	4.684587
244.313792	7566.074218	8.985741	-0.050326	4.687010
244.448047	7574.022106	8.990746	-0.050356	4.689398
244.635580	7582.114836	8.995751	-0.050396	4.691827
244.786630	7590.084659	9.000755	-0.050430	4.694219
244.891851	7598.154098	9.005760	-0.050454	4.696639
244.960887	7606.090005	9.010765	-0.050473	4.699018
245.260696	7614.140989	9.015770	-0.050534	4.701430
245.432549	7622.132760	9.020775	-0.050571	4.703823
245.354420	7630.168586	9.025779	-0.050562	4.706228
245.651672	7638.223833	9.030784	-0.050622	4.708637
245.682019	7646.188334	9.035789	-0.050633	4.711019
245.808234	7654.285114	9.040794	-0.050662	4.713438
245.898026	7662.324137	9.045799	-0.050684	4.715839
245.939197	7670.294728	9.050803	-0.050697	4.718219
246.031176	7678.300144	9.055808	-0.050719	4.720608
246.092456	7686.266465	9.060813	-0.050736	4.722984
246.623136	7694.269260	9.065818	-0.050840	4.725368
246.579165	7702.321427	9.070823	-0.050837	4.727767
246.779129	7710.343224	9.075827	-0.050879	4.730155
247.203971	7718.412198	9.080832	-0.050964	4.732556
247.212913	7726.414259	9.085837	-0.050971	4.734936
247.126641	7734.448830	9.090842	-0.050960	4.737326
247.596098	7742.391069	9.095847	-0.051053	4.739685
247.867823	7750.441617	9.100851	-0.051108	4.742075
247.809478	7758.453990	9.105856	-0.051103	4.744454
247.890444	7766.477107	9.110861	-0.051123	4.746835
248.176510	7774.442276	9.115866	-0.051182	4.749196
248.245107	7782.511322	9.120871	-0.051200	4.751588
248.224705	7790.588743	9.125875	-0.051201	4.753981
248.474437	7798.553094	9.130880	-0.051253	4.756339
248.570904	7806.518672	9.135885	-0.051276	4.758696
248.946076	7814.534801	9.140890	-0.051351	4.761067
248.959430	7822.526460	9.145895	-0.051359	4.763430
248.909119	7830.556195	9.150899	-0.051355	4.765803
249.213320	7838.557297	9.155904	-0.051417	4.768165
249.612829	7846.626091	9.160909	-0.051496	4.770546
249.585337	7854.618506	9.165914	-0.051497	4.772905
249.681487	7862.674701	9.170919	-0.051520	4.775281
249.728792	7870.636860	9.175923	-0.051534	4.777628
250.047121	7878.688173	9.180928	-0.051598	4.779999
250.011290	7886.667787	9.185933	-0.051597	4.782349
250.141629	7894.649354	9.190938	-0.051626	4.784698
250.343907	7902.720811	9.195943	-0.051669	4.787072
250.304964	7910.638986	9.200947	-0.051667	4.789401
250.363563	7918.780196	9.205952	-0.051684	4.791794
250.384798	7926.743200	9.210957	-0.051693	4.794133
250.792434	7934.832764	9.215962	-0.051774	4.796507
250.736984	7942.736602	9.220967	-0.051769	4.798827
250.782942	7950.799070	9.225971	-0.051783	4.801192
251.078568	7958.757520	9.230976	-0.051843	4.803524
251.334620	7966.824838	9.235981	-0.051896	4.805887
251.303136	7974.850153	9.240986	-0.051895	4.808238
251.572010	7982.846821	9.245991	-0.051951	4.810578
251.671355	7990.386969	9.250995	-0.051974	4.812784
251.893763	7995.102596	9.256000	-0.052019	4.814162

251.871595	7997.629057	9.261005	-0.052016	4.814901
251.950513	7999.073802	9.266010	-0.052032	4.815323
251.971154	7999.549272	9.271015	-0.052036	4.815462
251.998356	8000.298212	9.276019	-0.052042	4.815681
252.266124	8000.437114	9.281024	-0.052092	4.815720
252.294322	8000.504847	9.286029	-0.052097	4.815740
252.308710	8000.506152	9.291034	-0.052100	4.815740
252.350888	8000.434231	9.296039	-0.052107	4.815719
252.294295	8000.588143	9.301043	-0.052097	4.815764
252.496738	8000.431272	9.306048	-0.052135	4.815717
252.412892	8000.549503	9.311053	-0.052119	4.815752
252.530259	8000.440366	9.316058	-0.052141	4.815720
252.749720	8000.541112	9.321063	-0.052182	4.815748
252.582418	8000.394237	9.326067	-0.052151	4.815706
252.649787	8000.535219	9.331072	-0.052163	4.815747
252.832344	8000.513635	9.336077	-0.052197	4.815740
252.952020	8000.418416	9.341082	-0.052220	4.815711
252.801324	8000.534492	9.346087	-0.052192	4.815746
252.754044	8000.377825	9.351091	-0.052183	4.815700
252.690919	8000.324478	9.356096	-0.052171	4.815685
252.609067	8000.381877	9.361101	-0.052156	4.815702
252.831219	8000.425005	9.366106	-0.052197	4.815714
252.852272	8000.408266	9.371111	-0.052201	4.815709
252.807163	8000.447043	9.376115	-0.052193	4.815720
252.834044	8000.591639	9.381120	-0.052198	4.815763
253.065787	8000.566585	9.386125	-0.052241	4.815754
253.158974	8000.427153	9.391130	-0.052258	4.815713
252.969173	8000.458235	9.396135	-0.052223	4.815723
252.969632	8000.516975	9.401139	-0.052223	4.815740
253.208583	8000.513395	9.406144	-0.052268	4.815738
253.216452	8000.438778	9.411149	-0.052269	4.815716
253.108545	8000.358006	9.416154	-0.052249	4.815693
253.240815	8000.474419	9.421159	-0.052274	4.815726
253.196687	8000.420312	9.426163	-0.052266	4.815711
253.187426	8000.404147	9.431168	-0.052264	4.815706
253.224770	8000.441064	9.436173	-0.052271	4.815717
253.337090	8000.494151	9.441178	-0.052292	4.815732
253.139938	8000.417264	9.446183	-0.052255	4.815710
253.038158	8000.442305	9.451187	-0.052236	4.815718
253.208439	8000.215501	9.456192	-0.052268	4.815651
253.250844	8000.505572	9.461197	-0.052276	4.815735
253.275350	8000.392785	9.466202	-0.052281	4.815702
253.382202	8000.301628	9.471207	-0.052300	4.815675
253.388073	8000.498205	9.476211	-0.052302	4.815733
253.394314	8000.536751	9.481216	-0.052303	4.815744
253.335166	8000.402313	9.486221	-0.052292	4.815705
253.271948	8000.383133	9.491226	-0.052280	4.815700
253.371054	8000.536381	9.496231	-0.052299	4.815744
253.243462	8000.510813	9.501235	-0.052275	4.815737
253.626851	8000.467940	9.506240	-0.052346	4.815723
253.565477	8000.393264	9.511245	-0.052335	4.815701
253.547415	8000.362005	9.516250	-0.052332	4.815692
253.631718	8000.223497	9.521255	-0.052347	4.815651
253.358132	8000.449693	9.526259	-0.052296	4.815719
253.379372	8000.401990	9.531264	-0.052300	4.815705
253.463665	8000.423654	9.536269	-0.052316	4.815710
253.585646	8000.231301	9.541274	-0.052339	4.815654
253.593126	8000.372377	9.546279	-0.052340	4.815695
253.389426	8000.377605	9.551283	-0.052302	4.815697
253.496031	8000.506415	9.556288	-0.052322	4.815734
253.431769	8000.560899	9.561293	-0.052310	4.815751
253.506405	8000.422232	9.566298	-0.052324	4.815710
253.594896	8000.486678	9.571303	-0.052341	4.815728
253.463993	8000.404461	9.576307	-0.052316	4.815705
253.561027	8000.213837	9.581312	-0.052334	4.815649
253.425794	8000.298131	9.586317	-0.052309	4.815674
253.625921	8000.308868	9.591322	-0.052347	4.815676
253.551966	8000.355718	9.596327	-0.052333	4.815690
253.425535	8000.365408	9.601331	-0.052309	4.815694
253.749203	8000.334376	9.606336	-0.052370	4.815683
253.614191	8000.535067	9.611341	-0.052345	4.815742
253.364069	8000.390043	9.616346	-0.052298	4.815701
253.636574	8000.380602	9.621351	-0.052349	4.815697
253.713854	8000.519614	9.626355	-0.052363	4.815737
253.660830	8000.507006	9.631360	-0.052354	4.815734
253.801284	8000.470855	9.636365	-0.052380	4.815723
253.725046	8000.421564	9.641370	-0.052365	4.815709
253.748520	8000.304488	9.646375	-0.052370	4.815674
253.703314	8000.438301	9.651379	-0.052362	4.815714
253.846593	8000.186495	9.656384	-0.052388	4.815639
253.729149	8000.390675	9.661389	-0.052366	4.815700
253.820386	8000.276839	9.666394	-0.052383	4.815666
253.815838	8000.388889	9.671399	-0.052383	4.815699
253.633260	8000.519397	9.676403	-0.052349	4.815738
253.705187	8000.301667	9.681408	-0.052362	4.815674
253.592408	8000.460006	9.686413	-0.052341	4.815720
253.672834	8000.299010	9.691418	-0.052356	4.815673
253.815736	8000.222321	9.696423	-0.052383	4.815650
253.495378	8000.368737	9.701427	-0.052323	4.815694
253.834554	8000.382807	9.706432	-0.052386	4.815697
253.788573	8000.363908	9.711437	-0.052378	4.815691
253.619284	8000.447647	9.716442	-0.052346	4.815717
253.608107	8000.357771	9.721447	-0.052344	4.815690
253.703530	8000.395634	9.726451	-0.052362	4.815701
253.821178	8000.266210	9.731456	-0.052384	4.815663
253.745140	8000.608816	9.736461	-0.052370	4.815763
253.762988	8000.429713	9.741466	-0.052373	4.815711
253.807289	8000.283078	9.746471	-0.052381	4.815668
253.819230	8000.549165	9.751475	-0.052384	4.815745
253.835103	8000.373234	9.756480	-0.052387	4.815694
253.828703	8000.632616	9.761485	-0.052386	4.815770
253.827383	8000.376317	9.766490	-0.052385	4.815695
253.734570	8000.391893	9.771495	-0.052368	4.815700
253.717983	8000.597718	9.776499	-0.052365	4.815760
253.690534	8000.456319	9.781504	-0.052360	4.815719
253.779594	8000.493011	9.786509	-0.052377	4.815729
253.973352	8000.459864	9.791514	-0.052413	4.815719
254.147077	8000.536378	9.796519	-0.052445	4.815740
253.929720	8000.603317	9.801523	-0.052405	4.815761
254.041197	8000.433214	9.806528	-0.052425	4.815710
254.165866	8000.528150	9.811533	-0.052449	4.815738
254.215159	8000.347423	9.816538	-0.052458	4.815685
254.019598	8000.452092	9.821543	-0.052422	4.815716
254.022122	8000.242841	9.826547	-0.052422	4.815655
254.117133	8000.323410	9.831552	-0.052440	4.815678
253.935875	8000.323664	9.836557	-0.052406	4.815679
254.016949	8000.299360	9.841562	-0.052421	4.815671
254.153423	8000.517289	9.846567	-0.052447	4.815734
253.937260	8000.505227	9.851571	-0.052406	4.815732
253.907842	8000.379814	9.856576	-0.052401	4.815695
254.029615	8000.366851	9.861581	-0.052424	4.815691
254.198636	8000.552208	9.866586	-0.052455	4.815744
254.114041	8000.420555	9.871591	-0.052439	4.815706
253.962330	8000.534481	9.876595	-0.052411	4.815740
253.965785	8000.261175	9.881600	-0.052412	4.815660
253.883538	8000.499033	9.886605	-0.052397	4.815730
253.965315	8000.498232	9.891610	-0.052412	4.815730
254.207270	8000.280066	9.896615	-0.052457	4.815665
254.005296	8000.420937	9.901619	-0.052419	4.815707
254.003923	8000.239386	9.906624	-0.052419	4.815654
254.066260	8000.523380	9.911629	-0.052431	4.815737
254.093570	8000.410637	9.916634	-0.052436	4.815704
254.121191	8000.426039	9.921639	-0.052441	4.815708
254.047757	8000.541241	9.926643	-0.052427	4.815742
254.184394	8000.383293	9.931648	-0.052453	4.815695
254.209515	8000.513982	9.936653	-0.052458	4.815733
254.031353	8000.505743	9.941658	-0.052425	4.815732
254.300879	8000.419370	9.946663	-0.052475	4.815705
254.206853	8000.511812	9.951667	-0.052457	4.815733
254.163832	8000.350937	9.956672	-0.052449	4.815686
254.138724	8000.528861	9.961677	-0.052445	4.815738
254.069435	8000.537345	9.966682	-0.052432	4.815741
254.175927	8000.369296	9.971687	-0.052452	4.815691
254.151237	8000.487427	9.976691	-0.052447	4.815726
254.209246	8000.331402	9.981696	-0.052458	4.815680
254.156274	8000.363645	9.986701	-0.052448	4.815690
254.103352	8000.426856	9.991706	-0.052438	4.815708
254.297673	8000.060555	9.996711	-0.052474	4.815600
254.126983	8000.027880	10.001715	-0.052442	4.815592
254.154613	8000.295288	10.006720	-0.052448	4.815670
254.216707	8000.514142	10.011725	-0.052459	4.815733
254.162586	8000.358426	10.016730	-0.052449	4.815688
254.139700	8000.522503	10.021735	-0.052445	4.815736
254.055636	8000.515797	10.026739	-0.052430	4.815734
254.253678	8000.314001	10.031744	-0.052466	4.815675
254.175023	8000.393879	10.036749	-0.052452	4.815698
254.236976	8000.315871	10.041754	-0.052463	4.815675
254.444495	8000.400410	10.046759	-0.052502	4.815699
254.395667	8000.498927	10.051763	-0.052493	4.815728
254.194732	8000.402754	10.056768	-0.052456	4.815701
254.250859	8000.514727	10.061773	-0.052466	4.815733
254.581952	8000.510514	10.066778	-0.052528	4.815730
254.699338	8000.425933	10.071783	-0.052550	4.815705
254.546624	8000.504605	10.076787	-0.052521	4.815729
254.482862	8000.303881	10.081792	-0.052509	4.815670
254.278683	8000.408410	10.086797	-0.052471	4.815702
254.411215	8000.352908	10.091802	-0.052496	4.815685
254.564760	8000.334055	10.096807	-0.052525	4.815679
254.351229	8000.438432	10.101811	-0.052485	4.815710
254.424424	8000.374489	10.106816	-0.052499	4.815691
254.416496	8000.404262	10.111821	-0.052497	4.815700
254.341358	8000.369937	10.116826	-0.052483	4.815690
254.274670	8000.144609	10.121831	-0.052471	4.815625
254.294444	8000.418300	10.126835	-0.052475	4.815705
254.483497	8000.299648	10.131840	-0.052510	4.815669
254.395415	8000.490428	10.136845	-0.052494	4.815725
254.304889	8000.526331	10.141850	-0.052477	4.815736
254.309830	8000.389730	10.146855	-0.052478	4.815696
254.439496	8000.374760	10.151859	-0.052502	4.815691
254.488150	8000.518647	10.156864	-0.052511	4.815733
254.416376	8000.526023	10.161869	-0.052498	4.815736
254.416629	8000.516419	10.166874	-0.052498	4.815733
254.353994	8000.420363	10.171879	-0.052486	4.815705
254.276357	8000.478900	10.176883	-0.052472	4.815723
254.426391	8000.377767	10.181888	-0.052500	4.815692
254.323464	8000.618494	10.186893	-0.052481	4.815763
254.165255	8000.403418	10.191898	-0.052451	4.815701
254.168206	8000.520931	10.196903	-0.052452	4.815735
254.237571	8000.601085	10.201907	-0.052465	4.815759
254.231943	8000.422666	10.206912	-0.052464	4.815706
254.421719	8000.501578	10.211917	-0.052499	4.815729
254.464104	8000.490525	10.216922	-0.052507	4.815725
254.509516	8000.310802	10.221927	-0.052515	4.815672
254.463521	8000.415772	10.226931	-0.052507	4.815703
254.613539	8000.132037	10.231936	-0.052535	4.815620
254.507199	8000.374843	10.236941	-0.052515	4.815691
254.419494	8000.442827	10.241946	-0.052499	4.815711
254.313413	8000.259569	10.246951	-0.052479	4.815658
254.458824	8000.513951	10.251955	-0.052506	4.815732
254.584447	8000.381452	10.256960	-0.052529	4.815693
254.332234	8000.549269	10.261965	-0.052483	4.815743
254.349822	8000.504709	10.266970	-0.052486	4.815730
254.358334	8000.425830	10.271975	-0.052487	4.815707
254.177413	8000.486956	10.276979	-0.052454	4.815725
254.313018	8000.496643	10.281984	-0.052479	4.815728
254.550117	8000.625448	10.286989	-0.052523	4.815764
254.287061	8000.515447	10.291994	-0.052474	4.815733
254.417953	8000.419340	10.296999	-0.052499	4.815705
254.417414	8000.576308	10.302003	-0.052499	4.815750
254.509512	8000.411227	10.307008	-0.052516	4.815702
254.510289	8000.424057	10.312013	-0.052516	4.815705
254.473350	8000.434136	10.317018	-0.052509	4.815709
254.461324	8000.504421	10.322023	-0.052507	4.815729
254.458302	8000.539614	10.327027	-0.052507	4.815739
254.473240	8000.428804	10.332032	-0.052509	4.815707
254.464833	8000.438280	10.337037	-0.052508	4.815710
254.365403	8000.502869	10.342042	-0.052489	4.815729
254.445893	8000.435841	10.347047	-0.052504	4.815709
254.501508	8000.567029	10.352051	-0.052515	4.815747
254.621461	8000.460065	10.357056	-0.052537	4.815715
254.475539	8000.424587	10.362061	-0.052510	4.815706
254.363681	8000.469752	10.367066	-0.052489	4.815720
254.436083	8000.348132	10.372071	-0.052503	4.815684
254.254961	8000.459444	10.377075	-0.052469	4.815717
254.367044	8000.400406	10.382080	-0.052490	4.815699
254.333100	8000.557897	10.387085	-0.052484	4.815745
254.429730	8000.392890	10.392090	-0.052502	4.815697
254.514183	8000.249042	10.397095	-0.052517	4.815654
254.340187	8000.547342	10.402099	-0.052485	4.815742
254.459331	8000.349599	10.407104	-0.052507	4.815684
254.472563	8000.389327	10.412109	-0.052510	4.815695
254.522568	8000.424316	10.417114	-0.052519	4.815705
254.752095	8000.306324	10.422119	-0.052562	4.815670
254.460635	8000.377395	10.427123	-0.052507	4.815692
254.518927	8000.087896	10.432128	-0.052518	4.815607
254.441227	8000.366406	10.437133	-0.052504	4.815689
254.240401	8000.306542	10.442138	-0.052467	4.815672
254.365858	8000.093955	10.447143	-0.052490	4.815610
254.445309	8000.256494	10.452147	-0.052505	4.815657
254.443181	8000.088813	10.457152	-0.052504	4.815608
254.499694	8000.322524	10.462157	-0.052515	4.815676
254.383637	8000.414606	10.467162	-0.052493	4.815703
254.758287	8000.263739	10.472167	-0.052563	4.815657
254.627164	8000.506143	10.477171	-0.052539	4.815729
254.650675	8000.184040	10.482176	-0.052543	4.815635
254.756322	8000.317108	10.487181	-0.052563	4.815673
254.701823	8000.261763	10.492186	-0.052553	4.815657
254.666736	8000.109561	10.497191	-0.052546	4.815613
254.492714	8000.527459	10.502195	-0.052514	4.815736
254.476989	8000.165207	10.507200	-0.052511	4.815630
254.454272	8000.393357	10.512205	-0.052507	4.815697
254.519309	8000.295110	10.517210	-0.052519	4.815668
254.644745	8000.156202	10.522215	-0.052542	4.815626
254.601721	8000.123469	10.527219	-0.052534	4.815617
254.581461	7999.971511	10.532224	-0.052530	4.815573
254.565169	8000.085505	10.537229	-0.052527	4.815606
254.610186	8000.303012	10.542234	-0.052536	4.815670
254.427558	8000.208206	10.547239	-0.052502	4.815643
254.383397	8000.417854	10.552243	-0.052494	4.815704
254.581147	8000.276919	10.557248	-0.052531	4.815662
254.500212	8000.282011	10.562253	-0.052516	4.815664
254.575590	8000.268292	10.567258	-0.052530	4.815660
254.706557	8000.105981	10.572263	-0.052554	4.815611
254.571849	8000.324832	10.577267	-0.052529	4.815676
254.595191	8000.073206	10.582272	-0.052533	4.815602
254.774602	8000.396483	10.587277	-0.052567	4.815696
254.619571	8000.433471	10.592282	-0.052538	4.815708
254.658423	8000.354018	10.597287	-0.052545	4.815684
254.693035	8000.407977	10.602291	-0.052552	4.815700
254.619386	8000.270096	10.607296	-0.052538	4.815660
254.648228	8000.512970	10.612301	-0.052544	4.815731
254.488613	8000.490083	10.617306	-0.052514	4.815725
254.558527	8000.465596	10.622311	-0.052527	4.815717
254.484078	8000.429147	10.627315	-0.052513	4.815707
254.421877	8000.440951	10.632320	-0.052502	4.815711
254.629141	8000.418702	10.637325	-0.052540	4.815703
254.552450	8000.438812	10.642330	-0.052526	4.815710
254.482769	8000.424866	10.647335	-0.052513	4.815706
254.426834	8000.562778	10.652339	-0.052503	4.815746
254.628139	8000.282013	10.657344	-0.052540	4.815663
254.601951	8000.169466	10.662349	-0.052535	4.815631
254.458264	8000.169264	10.667354	-0.052508	4.815631
254.649267	8000.174514	10.672359	-0.052544	4.815632
254.630165	8000.298075	10.677363	-0.052541	4.815668
254.660109	8000.121304	10.682368	-0.052546	4.815616
254.650375	8000.435094	10.687373	-0.052545	4.815708
254.500388	8000.363243	10.692378	-0.052517	4.815688
254.431024	8000.123989	10.697383	-0.052504	4.815618
254.417469	8000.421697	10.702387	-0.052501	4.815705
254.621870	8000.416488	10.707392	-0.052539	4.815703
254.660112	8000.413910	10.712397	-0.052547	4.815702
254.504632	8000.422058	10.717402	-0.052518	4.815705
254.646900	8000.129654	10.722407	-0.052544	4.815619
254.453611	8000.206596	10.727411	-0.052508	4.815642
254.436656	8000.105947	10.732416	-0.052505	4.815613
254.693351	8000.227593	10.737421	-0.052553	4.815647
254.609538	8000.209145	10.742426	-0.052537	4.815642
254.501242	8000.254368	10.747431	-0.052517	4.815656
254.170368	8000.418768	10.752435	-0.052456	4.815705
254.327844	8000.504628	10.757440	-0.052485	4.815730
254.562936	8000.465748	10.762445	-0.052529	4.815717
254.449150	8000.365654	10.767450	-0.052508	4.815689
254.740479	8000.172852	10.772455	-0.052562	4.815631
254.612855	8000.411041	10.777459	-0.052538	4.815701
254.685223	8000.366306	10.782464	-0.052552	4.815688
254.583930	8000.469307	10.787469	-0.052533	4.815718
254.597349	8000.388372	10.792474	-0.052535	4.815695
254.648371	8000.334746	10.797479	-0.052545	4.815679
254.782846	8000.450132	10.802483	-0.052570	4.815712
254.765396	8000.228806	10.807488	-0.052567	4.815647
254.568981	8000.203185	10.812493	-0.052530	4.815641
254.413050	8000.362959	10.817498	-0.052501	4.815688
254.595568	8000.269829	10.822503	-0.052535	4.815660
254.535697	8000.424762	10.827507	-0.052524	4.815705
254.549564	8000.439941	10.832512	-0.052527	4.815710
254.538047	8000.320157	10.837517	-0.052525	4.815675
254.658371	8000.256982	10.842522	-0.052547	4.815656
254.692829	8000.160373	10.847527	-0.052553	4.815627
254.400265	8000.299768	10.852531	-0.052499	4.815670
254.613517	8000.288295	10.857536	-0.052539	4.815665
254.722109	8000.253760	10.862541	-0.052559	4.815655
254.573782	8000.433948	10.867546	-0.052531	4.815708
254.574568	8000.062356	10.872551	-0.052531	4.815599
254.587127	8000.398932	10.877555	-0.052534	4.815698
254.654605	8000.307132	10.882560	-0.052547	4.815670
254.638845	8000.523652	10.887565	-0.052544	4.815734
254.697052	8000.460532	10.892570	-0.052555	4.815715
254.902883	8000.525825	10.897575	-0.052593	4.815733
254.738825	8000.439861	10.902579	-0.052562	4.815709
254.774088	8000.285600	10.907584	-0.052569	4.815664
254.856321	8000.109680	10.912589	-0.052584	4.815612
254.937535	8000.442040	10.917594	-0.052600	4.815709
254.855689	8000.183357	10.922599	-0.052584	4.815633
254.939549	8000.381210	10.927603	-0.052600	4.815691
255.011906	8000.205128	10.932608	-0.052613	4.815639
255.079633	8000.079161	10.937613	-0.052626	4.815602
254.783467	8000.364793	10.942618	-0.052571	4.815687
254.803291	8000.160093	10.947623	-0.052575	4.815627
254.604408	8000.360814	10.952627	-0.052538	4.815686
254.861775	8000.320160	10.957632	-0.052586	4.815673
255.100169	8000.333658	10.962637	-0.052630	4.815676
254.948765	8000.419826	10.967642	-0.052602	4.815702
254.891379	7999.999231	10.972647	-0.052591	4.815579
255.004081	8000.264826	10.977651	-0.052612	4.815656
255.079645	7999.988421	10.982656	-0.052626	4.815575
254.826227	8000.118843	10.987661	-0.052579	4.815615
254.769825	8000.330428	10.992666	-0.052569	4.815677
254.815345	8000.291662	10.997671	-0.052577	4.815665
254.889463	8000.406065	11.002675	-0.052591	4.815698
254.878390	8000.204064	11.007680	-0.052589	4.815639
254.925615	8000.329774	11.012685	-0.052598	4.815676
254.847595	8000.362677	11.017690	-0.052583	4.815686
254.865104	8000.348015	11.022695	-0.052587	4.815681
254.917646	8000.376639	11.027699	-0.052596	4.815690
254.934635	8000.271201	11.032704	-0.052600	4.815659
254.706231	8000.335825	11.037709	-0.052557	4.815679
254.893241	8000.299364	11.042714	-0.052592	4.815667
255.134039	8000.127095	11.047719	-0.052637	4.815616
254.850720	8000.230335	11.052723	-0.052584	4.815647
254.962335	8000.237495	11.057728	-0.052605	4.815649
255.025581	8000.291921	11.062733	-0.052617	4.815664
255.091247	8000.358133	11.067738	-0.052629	4.815683
254.977596	8000.361623	11.072743	-0.052608	4.815685
254.960855	8000.289807	11.077747	-0.052605	4.815664
255.014287	8000.325919	11.082752	-0.052615	4.815674
255.076996	8000.092017	11.087757	-0.052626	4.815606
254.818463	8000.366516	11.092762	-0.052578	4.815687
254.915745	8000.352086	11.097767	-0.052597	4.815682
254.951154	8000.395381	11.102771	-0.052603	4.815695
254.871908	8000.472046	11.107776	-0.052589	4.815718
254.862505	8000.361906	11.112781	-0.052587	4.815685
255.013741	8000.433784	11.117786	-0.052615	4.815706
254.918170	8000.331851	11.122791	-0.052597	4.815676
254.817628	8000.362251	11.127795	-0.052578	4.815686
254.723684	8000.214428	11.132800	-0.052561	4.815643
254.665391	8000.180379	11.137805	-0.052550	4.815633
254.654633	8000.083033	11.142810	-0.052548	4.815605
254.779186	8000.016723	11.147815	-0.052571	4.815585
254.785682	8000.199432	11.152819	-0.052573	4.815638
254.810489	8000.173143	11.157824	-0.052577	4.815631
254.818675	8000.060088	11.162829	-0.052579	4.815597
255.080508	8000.322775	11.167834	-0.052628	4.815673
254.980070	8000.031755	11.172839	-0.052609	4.815588
254.923589	8000.243339	11.177843	-0.052598	4.815651
254.738289	7999.984042	11.182848	-0.052564	4.815576
254.854262	8000.325507	11.187853	-0.052586	4.815675
254.697105	8000.079482	11.192858	-0.052556	4.815604
254.909238	8000.192927	11.197863	-0.052596	4.815636
254.709483	8000.492945	11.202867	-0.052559	4.815724
254.742721	8000.348262	11.207872	-0.052565	4.815682
255.016517	8000.269433	11.212877	-0.052616	4.815658
254.913795	8000.466384	11.217882	-0.052597	4.815716
254.782707	8000.159913	11.222887	-0.052572	4.815627
254.693543	8000.270587	11.227891	-0.052556	4.815660
254.733391	8000.310749	11.232896	-0.052563	4.815671
254.779559	8000.206855	11.237901	-0.052572	4.815641
254.779640	8000.410819	11.242906	-0.052572	4.815700
255.014084	8000.190392	11.247911	-0.052616	4.815635
254.741521	8000.431560	11.252915	-0.052565	4.815706
254.812912	8000.157221	11.257920	-0.052578	4.815626
254.934902	8000.306574	11.262925	-0.052601	4.815669
254.804025	8000.381330	11.267930	-0.052577	4.815691
254.842177	8000.322155	11.272935	-0.052584	4.815674
254.805283	8000.394171	11.277939	-0.052577	4.815695
254.888220	8000.189430	11.282944	-0.052593	4.815635
254.822270	8000.344264	11.287949	-0.052580	4.815680
254.757185	8000.431838	11.292954	-0.052568	4.815706
254.871061	8000.369625	11.297959	-0.052590	4.815688
254.783379	8000.483528	11.302963	-0.052573	4.815721
254.795427	8000.285106	11.307968	-0.052575	4.815663
254.929266	8000.462418	11.312973	-0.052601	4.815715
254.731696	8000.557444	11.317978	-0.052564	4.815743
254.742344	8000.369678	11.322983	-0.052566	4.815688
254.643674	8000.441755	11.327987	-0.052547	4.815710
254.691896	8000.192667	11.332992	-0.052556	4.815637
254.651162	8000.253941	11.337997	-0.052549	4.815655
254.609962	8000.463639	11.343002	-0.052541	4.815716
254.722553	8000.229481	11.348007	-0.052562	4.815647
254.652737	8000.283875	11.353011	-0.052549	4.815664
254.533562	8000.203984	11.358016	-0.052527	4.815641
254.736119	8000.343970	11.363021	-0.052565	4.815681
254.856941	8000.392928	11.368026	-0.052587	4.815695
254.910369	8000.190909	11.373031	-0.052597	4.815635
254.807160	8000.407072	11.378035	-0.052578	4.815699
254.851989	8000.408873	11.383040	-0.052587	4.815699
255.023528	8000.518458	11.388045	-0.052619	4.815730
254.662705	8000.197565	11.393050	-0.052551	4.815638
254.842594	8000.249619	11.398055	-0.052585	4.815653
254.899077	8000.499352	11.403059	-0.052596	4.815725
254.670865	7999.925409	11.408064	-0.052553	4.815559
254.692883	7999.820057	11.413069	-0.052557	4.815528
254.790623	8000.056572	11.418074	-0.052575	4.815596
254.651932	8000.178185	11.423079	-0.052549	4.815633
254.505215	8000.437419	11.428083	-0.052522	4.815709
254.669561	8000.439032	11.433088	-0.052553	4.815709
254.749257	8000.418977	11.438093	-0.052568	4.815703
254.550489	8000.466998	11.443098	-0.052531	4.815718
254.844666	8000.283852	11.448103	-0.052586	4.815663
255.019339	8000.628417	11.453107	-0.052618	4.815763
254.848309	8000.520981	11.458112	-0.052586	4.815732
254.840024	8000.248546	11.463117	-0.052585	4.815652
254.783192	8000.597880	11.468122	-0.052574	4.815755
255.121122	8000.429328	11.473127	-0.052637	4.815704
254.980911	8000.476167	11.478131	-0.052611	4.815718
254.831587	8000.379765	11.483136	-0.052583	4.815691
254.896299	8000.479066	11.488141	-0.052596	4.815720
254.795130	8000.546831	11.493146	-0.052577	4.815740
254.637610	8000.389427	11.498151	-0.052547	4.815695
254.828265	8000.471558	11.503155	-0.052583	4.815718
254.643804	8000.443994	11.508160	-0.052549	4.815710
254.719923	8000.420677	11.513165	-0.052563	4.815703
254.854266	8000.386562	11.518170	-0.052588	4.815693
254.917787	8000.212472	11.523175	-0.052600	4.815641
254.735120	8000.465783	11.528179	-0.052566	4.815716
254.794379	8000.282013	11.533184	-0.052577	4.815662
254.908775	8000.340476	11.538189	-0.052598	4.815679
254.712769	8000.489988	11.543194	-0.052562	4.815724
254.818980	8000.349697	11.548199	-0.052581	4.815682
254.866934	8000.439113	11.553203	-0.052590	4.815708
254.717293	8000.433474	11.558208	-0.052563	4.815707
254.730602	8000.263905	11.563213	-0.052565	4.815657
254.793376	8000.408023	11.568218	-0.052577	4.815699
254.929059	8000.298112	11.573223	-0.052602	4.815666
254.611343	8000.483016	11.578227	-0.052543	4.815722
254.647373	8000.438756	11.583232	-0.052550	4.815709
254.858941	8000.519092	11.588237	-0.052589	4.815731
254.851803	8000.532861	11.593242	-0.052588	4.815735
254.943897	8000.391271	11.598247	-0.052605	4.815694
254.821973	8000.543059	11.603251	-0.052582	4.815739
254.939407	8000.422172	11.608256	-0.052604	4.815703
254.823103	8000.435229	11.613261	-0.052583	4.815707
254.824681	8000.466226	11.618266	-0.052583	4.815716
254.921592	8000.310833	11.623271	-0.052601	4.815670
254.871887	8000.165866	11.628275	-0.052592	4.815628
254.772648	8000.198424	11.633280	-0.052573	4.815638
254.850867	8000.345996	11.638285	-0.052588	4.815681
254.651740	8000.504000	11.643290	-0.052551	4.815728
254.706235	8000.319084	11.648295	-0.052561	4.815674
254.839277	8000.559387	11.653299	-0.052586	4.815743
254.803564	8000.436004	11.658304	-0.052579	4.815707
254.716644	8000.107830	11.663309	-0.052563	4.815612
254.759666	8000.408598	11.668314	-0.052571	4.815700
255.064989	8000.342030	11.673319	-0.052628	4.815679
254.859600	8000.365382	11.678323	-0.052590	4.815686
254.816292	8000.391376	11.683328	-0.052582	4.815694
255.000125	8000.469125	11.688333	-0.052616	4.815716
254.892312	8000.496203	11.693338	-0.052596	4.815724
254.869211	8000.265172	11.698343	-0.052592	4.815657
254.785586	8000.297984	11.703347	-0.052576	4.815667
254.844535	8000.270115	11.708352	-0.052587	4.815659
254.924834	8000.302394	11.713357	-0.052602	4.815668
254.934668	8000.452057	11.718362	-0.052604	4.815711
254.904585	8000.352259	11.723367	-0.052599	4.815682
255.015340	8000.485413	11.728371	-0.052619	4.815721
254.841485	8000.459090	11.733376	-0.052587	4.815714
254.938762	8000.139254	11.738381	-0.052605	4.815620
254.585131	8000.555296	11.743386	-0.052539	4.815743
254.791225	7999.984156	11.748391	-0.052577	4.815575
254.632166	8000.416179	11.753395	-0.052548	4.815702
254.681810	8000.277103	11.758400	-0.052557	4.815661
254.816476	8000.532381	11.763405	-0.052582	4.815735
254.715680	8000.403666	11.768410	-0.052564	4.815698
255.037109	8000.218829	11.773415	-0.052623	4.815643
254.891434	8000.187627	11.778419	-0.052596	4.815634
254.906878	8000.328837	11.783424	-0.052599	4.815675
254.870744	8000.430765	11.788429	-0.052593	4.815705
255.017509	8000.530336	11.793434	-0.052620	4.815734
254.951839	8000.433160	11.798439	-0.052608	4.815706
254.854022	8000.508455	11.803443	-0.052590	4.815728
254.969433	8000.509271	11.808448	-0.052611	4.815728
255.008225	8000.469327	11.813453	-0.052618	4.815716
254.910445	8000.362018	11.818458	-0.052600	4.815685
254.871645	8000.155294	11.823463	-0.052593	4.815625
254.781070	8000.324677	11.828467	-0.052576	4.815675
254.978106	8000.335365	11.833472	-0.052613	4.815677
255.161714	8000.103432	11.838477	-0.052647	4.815608
255.083957	8000.308264	11.843482	-0.052633	4.815669
254.815333	8000.187494	11.848487	-0.052583	4.815635
254.948808	8000.229182	11.853491	-0.052608	4.815646
254.907149	8000.217828	11.858496	-0.052600	4.815643
254.904592	8000.270113	11.863501	-0.052599	4.815658
254.943235	8000.422381	11.868506	-0.052607	4.815703
255.090720	7999.964544	11.873511	-0.052634	4.815568
254.883731	8000.310360	11.878515	-0.052596	4.815670
254.899174	8000.287122	11.883520	-0.052599	4.815663
254.906358	8000.258410	11.888525	-0.052600	4.815655
254.871007	8000.518394	11.893530	-0.052593	4.815731
254.935691	8000.243944	11.898535	-0.052605	4.815651
254.781705	8000.371715	11.903539	-0.052577	4.815689
254.677852	8000.293141	11.908544	-0.052557	4.815666
254.922450	8000.360132	11.913549	-0.052603	4.815685
254.858656	8000.468017	11.918554	-0.052591	4.815716
255.032806	8000.108855	11.923559	-0.052624	4.815611
254.939155	8000.378566	11.928563	-0.052606	4.815690
254.891498	8000.329739	11.933568	-0.052597	4.815676
254.985059	8000.203124	11.938573	-0.052615	4.815638
254.950632	8000.356337	11.943578	-0.052609	4.815683
254.890880	8000.492052	11.948583	-0.052598	4.815723
255.060985	8000.420077	11.953587	-0.052629	4.815701
254.997759	8000.313331	11.958592	-0.052617	4.815670
254.966355	8000.239141	11.963597	-0.052611	4.815649
254.805951	8000.523783	11.968602	-0.052582	4.815733
254.820088	8000.394805	11.973607	-0.052584	4.815695
254.922797	8000.461621	11.978611	-0.052604	4.815714
254.950048	8000.507986	11.983616	-0.052609	4.815728
254.870956	8000.136155	11.988621	-0.052594	4.815619
254.837132	8000.438877	11.993626	-0.052588	4.815708
254.818198	8000.529339	11.998631	-0.052584	4.815734
254.830879	8000.449459	12.003635	-0.052587	4.815711
254.760501	8000.402397	12.008640	-0.052574	4.815698
254.997640	8000.160658	12.013645	-0.052618	4.815626
254.830967	8000.275409	12.018650	-0.052587	4.815660
254.985710	8000.348411	12.023655	-0.052616	4.815681
255.131588	8000.454374	12.028659	-0.052643	4.815711
255.092385	8000.504995	12.033664	-0.052636	4.815726
255.146435	8000.491997	12.038669	-0.052646	4.815722
255.143099	8000.542135	12.043674	-0.052645	4.815737
254.861878	8000.509790	12.048679	-0.052593	4.815729
254.888769	8000.299863	12.053683	-0.052598	4.815667
254.941970	8000.424604	12.058688	-0.052608	4.815703
254.902249	8000.271256	12.063693	-0.052600	4.815659
254.788229	8000.492583	12.068698	-0.052579	4.815724
254.936579	8000.378607	12.073703	-0.052607	4.815690
255.131063	8000.257907	12.078707	-0.052643	4.815654
255.066400	8000.411696	12.083712	-0.052631	4.815699
255.031968	8000.289402	12.088717	-0.052625	4.815663
254.993877	8000.456438	12.093722	-0.052618	4.815712
255.067567	8000.378620	12.098727	-0.052631	4.815689
254.950638	8000.532625	12.103731	-0.052610	4.815735
255.048848	8000.410356	12.108736	-0.052628	4.815699
255.140764	8000.484472	12.113741	-0.052645	4.815720
255.132828	8000.329505	12.118746	-0.052644	4.815675
255.009693	8000.145967	12.123751	-0.052621	4.815621
255.044410	8000.341952	12.128755	-0.052627	4.815679
254.868827	8000.442676	12.133760	-0.052595	4.815709
255.093631	8000.364117	12.138765	-0.052636	4.815685
255.057258	8000.459635	12.143770	-0.052630	4.815713
255.119517	8000.092242	12.148775	-0.052641	4.815605
254.922168	8000.423267	12.153779	-0.052605	4.815703
254.940822	8000.380860	12.158784	-0.052608	4.815690
255.047742	8000.434930	12.163789	-0.052628	4.815706
254.902917	8000.550038	12.168794	-0.052601	4.815740
255.076102	8000.414041	12.173799	-0.052633	4.815700
255.157393	8000.380129	12.178803	-0.052649	4.815689
255.241494	8000.269377	12.183808	-0.052664	4.815656
255.216660	8000.099186	12.188813	-0.052659	4.815607
255.191732	8000.442633	12.193818	-0.052655	4.815707
255.185267	8000.316523	12.198823	-0.052654	4.815670
255.030076	8000.451751	12.203827	-0.052625	4.815711
255.000733	8000.297503	12.208832	-0.052620	4.815666
255.117387	8000.392311	12.213837	-0.052641	4.815693
255.185385	8000.510888	12.218842	-0.052654	4.815727
255.257637	8000.282477	12.223847	-0.052667	4.815660
255.214145	8000.368268	12.228851	-0.052659	4.815685
255.146751	8000.479298	12.233856	-0.052647	4.815718
255.220388	8000.364104	12.238861	-0.052661	4.815684
255.167361	8000.442264	12.243866	-0.052651	4.815707
255.303799	8000.191407	12.248871	-0.052676	4.815633
255.188072	8000.458625	12.253875	-0.052655	4.815712
255.147950	8000.142956	12.258880	-0.052647	4.815620
255.273549	8000.376731	12.263885	-0.052671	4.815688
255.109241	8000.504335	12.268890	-0.052640	4.815726
255.111857	8000.066560	12.273895	-0.052640	4.815598
255.281107	8000.261533	12.278899	-0.052672	4.815654
255.211811	8000.369329	12.283904	-0.052659	4.815686
255.312038	8000.247093	12.288909	-0.052678	4.815650
255.118672	8000.518386	12.293914	-0.052642	4.815730
255.316556	8000.301633	12.298919	-0.052679	4.815665
255.029722	8000.413358	12.303923	-0.052626	4.815700
255.226283	8000.327932	12.308928	-0.052662	4.815674
255.420470	8000.104713	12.313933	-0.052698	4.815607
255.178265	8000.467045	12.318938	-0.052653	4.815715
255.267931	8000.300855	12.323943	-0.052670	4.815665
255.368911	8000.397543	12.328947	-0.052689	4.815693
255.295865	8000.491396	12.333952	-0.052675	4.815721
255.351793	8000.241362	12.338957	-0.052686	4.815648
255.248060	8000.472469	12.343962	-0.052667	4.815716
255.380527	8000.180968	12.348967	-0.052691	4.815630
255.375093	8000.374165	12.353971	-0.052690	4.815686
255.434314	8000.275821	12.358976	-0.052701	4.815657
255.529459	8000.273103	12.363981	-0.052719	4.815656
255.422596	8000.126136	12.368986	-0.052699	4.815614
255.250893	7999.979182	12.373991	-0.052667	4.815572
255.237697	8000.316411	12.378995	-0.052665	4.815670
255.243021	8000.317569	12.384000	-0.052666	4.815670
255.184345	8000.093434	12.389005	-0.052655	4.815605
254.979096	8000.436077	12.394010	-0.052617	4.815706
255.302209	8000.264081	12.399015	-0.052677	4.815655
255.187545	8000.444820	12.404019	-0.052656	4.815708
255.019562	8000.484799	12.409024	-0.052624	4.815720
255.197044	8000.371297	12.414029	-0.052657	4.815686
255.252062	8000.163964	12.419034	-0.052668	4.815626
255.261050	8000.308274	12.424039	-0.052669	4.815668
255.050674	8000.476775	12.429043	-0.052630	4.815718
255.229809	8000.272531	12.434048	-0.052664	4.815657
255.141854	8000.329833	12.439053	-0.052647	4.815675
255.219167	8000.414389	12.444058	-0.052662	4.815699
255.333720	8000.293455	12.449063	-0.052683	4.815663
255.419536	8000.538331	12.454067	-0.052699	4.815734
255.251527	8000.488608	12.459072	-0.052668	4.815720
255.420235	8000.179544	12.464077	-0.052699	4.815629
255.410709	8000.246667	12.469082	-0.052698	4.815649
255.249855	8000.136195	12.474087	-0.052668	4.815617
255.279301	7999.914566	12.479091	-0.052673	4.815552
255.285644	8000.230755	12.484096	-0.052674	4.815645
255.254779	8000.092502	12.489101	-0.052669	4.815605
255.136251	8000.082031	12.494106	-0.052646	4.815602
255.345375	7999.947689	12.499111	-0.052685	4.815562
255.174264	8000.192645	12.504115	-0.052654	4.815634
254.940568	8000.242233	12.509120	-0.052610	4.815650
255.277042	8000.092879	12.514125	-0.052673	4.815605
255.312373	8000.285671	12.519130	-0.052680	4.815661
255.458190	8000.176993	12.524135	-0.052707	4.815628
255.345096	8000.088657	12.529139	-0.052686	4.815603
255.241037	8000.053861	12.534144	-0.052666	4.815593
255.466804	8000.074628	12.539149	-0.052708	4.815598
255.261060	8000.229321	12.544154	-0.052670	4.815645
255.277233	8000.080088	12.549159	-0.052673	4.815601
255.261674	8000.052073	12.554163	-0.052670	4.815593
255.134944	8000.311635	12.559168	-0.052647	4.815669
255.319835	8000.087197	12.564173	-0.052681	4.815603
255.185079	8000.417108	12.569178	-0.052656	4.815700
255.378794	8000.201356	12.574183	-0.052692	4.815636
255.262770	8000.179179	12.579187	-0.052671	4.815630
255.276298	8000.261627	12.584192	-0.052673	4.815654
255.351184	7999.849594	12.589197	-0.052687	4.815533
255.111715	8000.208762	12.594202	-0.052643	4.815639
255.393152	8000.027544	12.599207	-0.052695	4.815585
255.468259	8000.405726	12.604211	-0.052709	4.815695
255.351321	8000.262864	12.609216	-0.052687	4.815654
255.183575	8000.362648	12.614221	-0.052656	4.815684
255.240211	8000.426578	12.619226	-0.052667	4.815702
255.141075	8000.137712	12.624231	-0.052648	4.815618
255.358820	8000.474436	12.629235	-0.052689	4.815716
255.346520	8000.413369	12.634240	-0.052687	4.815698
255.433023	8000.192666	12.639245	-0.052703	4.815633
255.232224	8000.469177	12.644250	-0.052666	4.815715
255.103692	8000.158474	12.649255	-0.052641	4.815625
255.421731	8000.141233	12.654259	-0.052701	4.815618
255.055293	8000.413976	12.659264	-0.052633	4.815700
255.207764	8000.320356	12.664269	-0.052661	4.815671
255.397750	8000.369373	12.669274	-0.052696	4.815685
255.261656	8000.370362	12.674279	-0.052671	4.815686
255.284789	8000.230852	12.679283	-0.052675	4.815645
255.262120	8000.310575	12.684288	-0.052671	4.815668
255.449860	8000.305094	12.689293	-0.052706	4.815666
255.218451	8000.464709	12.694298	-0.052663	4.815714
255.157829	8000.182877	12.699303	-0.052652	4.815631
255.406552	8000.418659	12.704307	-0.052698	4.815699
255.427957	8000.451047	12.709312	-0.052702	4.815709
255.341838	8000.185883	12.714317	-0.052686	4.815631
255.322126	8000.386323	12.719322	-0.052683	4.815690
255.460129	8000.317028	12.724327	-0.052708	4.815669
255.205648	8000.414331	12.729331	-0.052661	4.815699
255.294386	8000.363454	12.734336	-0.052678	4.815684
255.421368	8000.321744	12.739341	-0.052701	4.815671
255.322923	8000.509155	12.744346	-0.052683	4.815726
255.289707	8000.264075	12.749351	-0.052677	4.815655
255.462732	8000.405720	12.754355	-0.052709	4.815695
255.545636	8000.345138	12.759360	-0.052725	4.815677
255.409370	8000.327970	12.764365	-0.052699	4.815673
255.524653	8000.409942	12.769370	-0.052721	4.815696
255.515864	8000.259232	12.774375	-0.052719	4.815652
255.451811	8000.283820	12.779379	-0.052707	4.815660
255.490607	8000.377359	12.784384	-0.052715	4.815687
255.527550	8000.154780	12.789389	-0.052721	4.815621
255.472454	8000.494535	12.794394	-0.052711	4.815721
255.596508	8000.218913	12.799399	-0.052734	4.815640
255.606664	8000.284222	12.804403	-0.052736	4.815659
255.583104	8000.461108	12.809408	-0.052732	4.815711
255.415734	8000.288591	12.814413	-0.052701	4.815661
255.300976	8000.294198	12.819418	-0.052679	4.815663
255.419945	8000.221390	12.824423	-0.052702	4.815641
255.443837	7999.992193	12.829427	-0.052706	4.815574
255.375901	8000.168353	12.834432	-0.052693	4.815626
255.576570	8000.121436	12.839437	-0.052731	4.815611
255.556753	8000.164898	12.844442	-0.052727	4.815624
255.619956	8000.029245	12.849447	-0.052739	4.815584
255.597560	7999.941319	12.854451	-0.052735	4.815559
255.423647	8000.365632	12.859456	-0.052703	4.815684
255.432445	7999.980281	12.864461	-0.052704	4.815571
255.311352	8000.306142	12.869466	-0.052682	4.815667
255.308689	8000.179027	12.874471	-0.052681	4.815630
255.219555	8000.303584	12.879475	-0.052665	4.815666
255.315791	8000.520865	12.884480	-0.052683	4.815729
255.603449	8000.396344	12.889485	-0.052736	4.815692
255.409116	8000.509578	12.894490	-0.052700	4.815726
255.276667	8000.494607	12.899495	-0.052675	4.815722
255.478374	8000.630315	12.904499	-0.052713	4.815761
255.417977	8000.486237	12.909504	-0.052702	4.815719
255.439968	8000.343504	12.914509	-0.052706	4.815677
255.193686	8000.149414	12.919514	-0.052660	4.815621
255.440414	8000.236730	12.924519	-0.052706	4.815646
255.433043	8000.182152	12.929523	-0.052705	4.815630
255.349539	8000.502222	12.934528	-0.052689	4.815724
255.508230	8000.450350	12.939533	-0.052719	4.815708
255.568294	8000.433178	12.944538	-0.052730	4.815703
255.697482	8000.105315	12.949543	-0.052754	4.815606
255.495762	8000.233377	12.954547	-0.052716	4.815645
255.441867	8000.364917	12.959552	-0.052707	4.815683
255.338668	8000.263927	12.964557	-0.052687	4.815654
255.364007	8000.482188	12.969562	-0.052692	4.815718
255.438281	8000.409718	12.974567	-0.052706	4.815696
255.399320	8000.271331	12.979571	-0.052699	4.815656
255.363021	8000.367918	12.984576	-0.052692	4.815685
255.324007	7999.990332	12.989581	-0.052685	4.815574
255.465548	8000.242518	12.994586	-0.052711	4.815647
255.648923	7999.927288	12.999591	-0.052745	4.815554
255.513065	8000.047880	13.004595	-0.052720	4.815590
255.625827	8000.318822	13.009600	-0.052741	4.815669
255.619807	8000.110493	13.014605	-0.052740	4.815608
255.627065	8000.023050	13.019610	-0.052741	4.815582
255.347476	8000.175472	13.024615	-0.052689	4.815628
255.501928	8000.294389	13.029619	-0.052718	4.815662
255.346213	8000.257682	13.034624	-0.052689	4.815652
255.482295	8000.115742	13.039629	-0.052714	4.815610
255.415407	8000.448896	13.044634	-0.052702	4.815708
255.415806	8000.397648	13.049639	-0.052702	4.815693
255.541355	8000.406104	13.054643	-0.052726	4.815695
255.557315	8000.452286	13.059648	-0.052729	4.815708
255.567296	8000.118209	13.064653	-0.052730	4.815611
255.313511	8000.256101	13.069658	-0.052683	4.815652
255.503333	8000.374527	13.074663	-0.052719	4.815686
255.679931	8000.228974	13.079667	-0.052752	4.815642
255.566595	8000.389446	13.084672	-0.052731	4.815690
255.735790	8000.046218	13.089677	-0.052762	4.815589
255.725482	8000.201961	13.094682	-0.052760	4.815634
255.637918	7999.982694	13.099687	-0.052744	4.815571
255.392026	8000.073729	13.104691	-0.052698	4.815598
255.301679	8000.073328	13.109696	-0.052681	4.815599
255.481785	8000.085876	13.114701	-0.052715	4.815601
255.442173	8000.043587	13.119706	-0.052707	4.815589
255.465614	7999.913695	13.124711	-0.052712	4.815551
255.608131	8000.044161	13.129715	-0.052738	4.815589
255.563334	8000.412915	13.134720	-0.052730	4.815697
255.601703	8000.269380	13.139725	-0.052737	4.815655
255.509709	8000.170708	13.144730	-0.052720	4.815626
255.461164	8000.098374	13.149735	-0.052711	4.815605
255.581838	8000.324594	13.154739	-0.052734	4.815671
255.641015	8000.410992	13.159744	-0.052745	4.815696
255.644470	8000.197477	13.164749	-0.052746	4.815633
255.536374	8000.290758	13.169754	-0.052725	4.815661
255.546697	8000.293065	13.174759	-0.052727	4.815662
255.614587	8000.293106	13.179763	-0.052740	4.815661
255.562465	8000.434287	13.184768	-0.052731	4.815703
255.595017	8000.111256	13.189773	-0.052736	4.815608
255.645640	8000.321385	13.194778	-0.052746	4.815670
255.725710	8000.134748	13.199783	-0.052761	4.815615
255.678261	7999.884100	13.204787	-0.052752	4.815542
255.672950	8000.086909	13.209792	-0.052751	4.815601
255.868642	7999.972636	13.214797	-0.052787	4.815567
255.599746	8000.131639	13.219802	-0.052737	4.815614
255.347743	8000.262086	13.224807	-0.052691	4.815654
255.545561	8000.303756	13.229811	-0.052728	4.815665
255.365950	8000.335003	13.234816	-0.052694	4.815675
255.595754	8000.212743	13.239821	-0.052737	4.815638
255.622841	8000.306092	13.244826	-0.052742	4.815665
255.601885	8000.210713	13.249831	-0.052738	4.815637
255.504901	7999.950715	13.254835	-0.052720	4.815562
255.524410	8000.240424	13.259840	-0.052724	4.815646
255.612062	8000.020808	13.264845	-0.052740	4.815582
255.574103	8000.262597	13.269850	-0.052733	4.815653
255.508516	8000.396083	13.274855	-0.052721	4.815692
255.691088	8000.400129	13.279859	-0.052755	4.815692
255.472844	8000.346385	13.284864	-0.052714	4.815678
255.315908	8000.284029	13.289869	-0.052685	4.815660
255.507648	8000.235899	13.294874	-0.052721	4.815645
255.465981	8000.039805	13.299879	-0.052713	4.815588
255.479575	7999.931109	13.304883	-0.052716	4.815556
255.494751	8000.201526	13.309888	-0.052719	4.815635
255.632442	7999.936809	13.314893	-0.052744	4.815557
255.702118	8000.197436	13.319898	-0.052757	4.815633
255.490173	8000.379794	13.324903	-0.052718	4.815687
255.613645	8000.435203	13.329907	-0.052741	4.815703
255.596413	8000.353766	13.334912	-0.052738	4.815679
255.541361	8000.284528	13.339917	-0.052727	4.815659
255.518560	8000.304449	13.344922	-0.052723	4.815665
255.586477	8000.461468	13.349927	-0.052736	4.815711
255.617962	8000.076484	13.354931	-0.052742	4.815598
255.556208	8000.379822	13.359936	-0.052730	4.815687
255.699342	8000.229452	13.364941	-0.052757	4.815642
255.692744	8000.500588	13.369946	-0.052756	4.815722
255.605516	8000.222589	13.374951	-0.052740	4.815641
255.611634	8000.244049	13.379955	-0.052741	4.815647
255.494650	8000.533675	13.384960	-0.052719	4.815732
255.627345	8000.191986	13.389965	-0.052744	4.815632
255.717876	8000.212685	13.394970	-0.052761	4.815637
255.525931	8000.377215	13.399975	-0.052725	4.815686
255.594760	8000.482992	13.404979	-0.052738	4.815717
255.614256	8000.476906	13.409984	-0.052742	4.815715
255.777052	8000.195507	13.414989	-0.052772	4.815632
255.666224	8000.582411	13.419994	-0.052751	4.815746
255.587613	8000.477548	13.424999	-0.052737	4.815715
255.834164	8000.330999	13.430003	-0.052783	4.815671
255.926402	8000.500163	13.435008	-0.052800	4.815720
255.817616	8000.416165	13.440013	-0.052780	4.815696
255.691297	8000.468571	13.445018	-0.052756	4.815712
255.805230	8000.457616	13.450023	-0.052777	4.815709
255.918642	8000.490437	13.455027	-0.052799	4.815718
255.728462	8000.532190	13.460032	-0.052763	4.815731
256.024757	8000.260442	13.465037	-0.052818	4.815650
255.944613	8000.496208	13.470042	-0.052804	4.815719
255.850785	8000.345178	13.475047	-0.052786	4.815675
255.680189	8000.270852	13.480051	-0.052754	4.815655
255.617492	8000.506902	13.485056	-0.052743	4.815724
255.788806	8000.426402	13.490061	-0.052775	4.815700
255.700395	8000.636406	13.495066	-0.052758	4.815761
255.739268	8000.401039	13.500071	-0.052765	4.815692
255.777570	8000.231874	13.505075	-0.052773	4.815643
255.620961	8000.495226	13.510080	-0.052744	4.815720
255.754539	8000.260337	13.515085	-0.052768	4.815651
255.727675	8000.251359	13.520090	-0.052763	4.815649
255.734271	8000.203415	13.525095	-0.052765	4.815635
255.841212	8000.176329	13.530099	-0.052784	4.815626
255.812032	8000.320019	13.535104	-0.052779	4.815668
255.720176	8000.196787	13.540109	-0.052762	4.815633
255.577818	8000.370668	13.545114	-0.052736	4.815684
255.618895	8000.014674	13.550119	-0.052743	4.815580
255.714386	8000.302420	13.555123	-0.052761	4.815664
255.635787	8000.388708	13.560128	-0.052747	4.815689
255.832560	8000.227465	13.565133	-0.052783	4.815641
255.915694	8000.512880	13.570138	-0.052799	4.815724
255.874151	8000.520748	13.575143	-0.052791	4.815727
255.974996	8000.521328	13.580147	-0.052810	4.815726
255.809355	8000.363786	13.585152	-0.052779	4.815681
255.840388	8000.003355	13.590157	-0.052785	4.815576
255.739926	8000.198208	13.595162	-0.052766	4.815633
255.955210	8000.332000	13.600167	-0.052806	4.815671
255.876173	8000.304018	13.605171	-0.052792	4.815663
255.683613	8000.240013	13.610176	-0.052756	4.815646
255.638653	8000.131429	13.615181	-0.052747	4.815614
255.775221	8000.427323	13.620186	-0.052773	4.815700
255.673227	8000.378676	13.625191	-0.052754	4.815686
255.650194	8000.061147	13.630195	-0.052749	4.815593
255.802759	8000.172558	13.635200	-0.052778	4.815625
255.932521	8000.032649	13.640205	-0.052802	4.815584
255.822491	8000.371510	13.645210	-0.052782	4.815683
255.928956	8000.233356	13.650215	-0.052802	4.815642
256.035605	8000.162482	13.655219	-0.052821	4.815621
255.867769	8000.325269	13.660224	-0.052790	4.815670
255.988990	8000.102995	13.665229	-0.052813	4.815604
255.907611	8000.317382	13.670234	-0.052798	4.815667
255.987416	8000.311210	13.675239	-0.052813	4.815665
255.787955	8000.145645	13.680243	-0.052776	4.815617
255.778636	8000.520321	13.685248	-0.052774	4.815727
255.889394	8000.405730	13.690253	-0.052795	4.815693
255.750280	8000.289202	13.695258	-0.052769	4.815660
255.904420	8000.152894	13.700263	-0.052797	4.815619
255.983181	8000.138162	13.705267	-0.052812	4.815614
255.723873	8000.387025	13.710272	-0.052764	4.815688
256.056824	8000.106264	13.715277	-0.052826	4.815605
256.234976	8000.070727	13.720282	-0.052859	4.815593
256.174613	8000.126343	13.725287	-0.052848	4.815610
256.030839	7999.956348	13.730291	-0.052821	4.815561
256.047982	8000.136032	13.735296	-0.052824	4.815613
256.002897	8000.370233	13.740301	-0.052816	4.815682
255.943551	8000.277430	13.745306	-0.052805	4.815655
255.987938	8000.240781	13.750311	-0.052813	4.815644
256.084875	8000.025586	13.755315	-0.052831	4.815581
256.010473	8000.544434	13.760320	-0.052818	4.815733
255.902019	8000.171045	13.765325	-0.052797	4.815624
256.044209	8000.035611	13.770330	-0.052824	4.815584
255.978638	8000.209675	13.775335	-0.052812	4.815635
256.001064	8000.077628	13.780339	-0.052816	4.815596
255.785653	8000.097613	13.785344	-0.052776	4.815603
256.099426	8000.004486	13.790349	-0.052834	4.815575
256.080381	8000.396089	13.795354	-0.052831	4.815689
256.121785	8000.358323	13.800359	-0.052839	4.815678
256.381236	8000.171404	13.805363	-0.052887	4.815622
256.112418	8000.263134	13.810368	-0.052837	4.815650
256.012220	8000.083169	13.815373	-0.052818	4.815598
256.242500	8000.154200	13.820378	-0.052861	4.815618
256.086074	8000.230677	13.825383	-0.052832	4.815641
256.165745	8000.412451	13.830387	-0.052847	4.815694
255.863702	8000.416072	13.835392	-0.052791	4.815696
256.078348	8000.133383	13.840397	-0.052831	4.815612
256.011860	8000.404611	13.845402	-0.052818	4.815692
255.916340	8000.198024	13.850407	-0.052801	4.815632
255.958694	8000.038537	13.855411	-0.052808	4.815585
255.807500	8000.020058	13.860416	-0.052780	4.815581
255.941652	7999.943225	13.865421	-0.052805	4.815557
256.011443	8000.178228	13.870426	-0.052818	4.815626
255.920089	8000.113737	13.875431	-0.052801	4.815607
256.025527	8000.209431	13.880435	-0.052821	4.815635
256.155211	8000.271349	13.885440	-0.052845	4.815652
256.172195	7999.987574	13.890445	-0.052848	4.815569
255.817208	8000.207112	13.895450	-0.052782	4.815635
255.690268	8000.085446	13.900455	-0.052759	4.815600
255.964129	8000.294943	13.905459	-0.052810	4.815660
255.997322	8000.357424	13.910464	-0.052816	4.815678
255.872055	8000.229375	13.915469	-0.052793	4.815641
255.873800	8000.152520	13.920474	-0.052793	4.815619
255.980663	8000.200182	13.925479	-0.052813	4.815632
255.890987	8000.404824	13.930483	-0.052796	4.815693
255.874556	8000.363980	13.935488	-0.052793	4.815681
256.011316	8000.193215	13.940493	-0.052819	4.815630
256.047208	8000.240790	13.945498	-0.052826	4.815644
255.925283	8000.355204	13.950503	-0.052803	4.815678
256.250488	8000.027330	13.955507	-0.052863	4.815581
256.128890	8000.392702	13.960512	-0.052841	4.815688
256.130535	8000.374577	13.965517	-0.052841	4.815683
256.041867	8000.111504	13.970522	-0.052825	4.815606
256.126471	8000.365973	13.975527	-0.052841	4.815680
256.224942	8000.154005	13.980531	-0.052859	4.815618
256.032716	8000.219219	13.985536	-0.052823	4.815638
256.151886	7999.939246	13.990541	-0.052845	4.815555
256.073336	8000.168628	13.995546	-0.052831	4.815623
256.055641	8000.122424	14.000551	-0.052827	4.815609
256.129457	7999.881225	14.005555	-0.052841	4.815538
255.997096	8000.305150	14.010560	-0.052817	4.815663
255.813753	8000.070437	14.015565	-0.052782	4.815595
255.829118	8000.278925	14.020570	-0.052785	4.815656
255.896693	8000.286436	14.025575	-0.052798	4.815658
256.073149	8000.114184	14.030579	-0.052831	4.815607
255.920207	8000.205667	14.035584	-0.052802	4.815634
255.957295	7999.851744	14.040589	-0.052809	4.815531
256.076008	8000.233841	14.045594	-0.052832	4.815642
255.983966	8000.320977	14.050599	-0.052815	4.815668
255.994749	8000.087291	14.055603	-0.052816	4.815599
256.251736	8000.327484	14.060608	-0.052864	4.815668
256.240057	8000.193811	14.065613	-0.052862	4.815629
255.942048	8000.294676	14.070618	-0.052807	4.815660
256.041205	8000.261055	14.075623	-0.052825	4.815650
256.103054	8000.212944	14.080627	-0.052837	4.815636
256.083016	8000.222231	14.085632	-0.052833	4.815638
256.176649	8000.172502	14.090637	-0.052851	4.815623
255.924915	8000.270918	14.095642	-0.052804	4.815653
255.772374	8000.420073	14.100647	-0.052776	4.815698
255.818485	8000.167741	14.105651	-0.052784	4.815624
255.893775	8000.538458	14.110656	-0.052798	4.815732
255.984072	8000.221703	14.115661	-0.052815	4.815639
255.966250	8000.465961	14.120666	-0.052812	4.815710
255.949126	8000.233954	14.125671	-0.052808	4.815642
256.023902	8000.399629	14.130675	-0.052823	4.815690
255.805883	8000.461219	14.135680	-0.052782	4.815710
255.973004	7999.976995	14.140685	-0.052813	4.815567
256.293585	8000.191525	14.145690	-0.052873	4.815628
256.173426	8000.093461	14.150695	-0.052850	4.815600
256.219927	7999.931905	14.155699	-0.052859	4.815553
256.179464	8000.260154	14.160704	-0.052852	4.815649
256.084057	8000.305588	14.165709	-0.052834	4.815663
255.923865	8000.088337	14.170714	-0.052804	4.815600
256.038419	8000.243980	14.175719	-0.052825	4.815645
256.112756	8000.160833	14.180723	-0.052839	4.815620
255.955163	8000.353689	14.185728	-0.052810	4.815677
255.972166	8000.169226	14.190733	-0.052813	4.815623
256.021833	8000.165767	14.195738	-0.052822	4.815622
255.896627	8000.371965	14.200743	-0.052799	4.815683
255.837389	7999.979094	14.205747	-0.052788	4.815568
255.801462	8000.418474	14.210752	-0.052782	4.815697
255.886896	8000.361136	14.215757	-0.052798	4.815680
255.813247	8000.350327	14.220762	-0.052784	4.815677
255.951385	8000.414519	14.225767	-0.052810	4.815695
256.090185	8000.237380	14.230771	-0.052835	4.815643
256.004741	8000.340643	14.235776	-0.052820	4.815673
255.994646	8000.345820	14.240781	-0.052818	4.815675
256.206411	8000.010758	14.245786	-0.052857	4.815576
256.246427	8000.107521	14.250791	-0.052865	4.815604
256.134613	7999.938047	14.255795	-0.052844	4.815555
256.021836	7999.549652	14.260800	-0.052822	4.815442

255.871440	7996.263961	14.265805	-0.052792	4.814482
255.942876	7990.706979	14.270810	-0.052802	4.812856
255.847718	7983.922327	14.275815	-0.052780	4.810872
255.999941	7976.668808	14.280819	-0.052804	4.808748
255.897705	7969.002006	14.285824	-0.052780	4.806503
255.929314	7961.223698	14.290829	-0.052780	4.804224
255.997866	7953.414499	14.295834	-0.052788	4.801935
255.929410	7945.363228	14.300839	-0.052770	4.799574
255.921902	7937.450890	14.305843	-0.052764	4.797252
255.924482	7929.358597	14.310848	-0.052759	4.794877
255.865857	7921.379965	14.315853	-0.052743	4.792534
255.735753	7913.396815	14.320858	-0.052713	4.790188
255.530149	7905.367738	14.325863	-0.052670	4.787829
255.878410	7897.426759	14.330867	-0.052730	4.785492
255.696719	7889.392165	14.335872	-0.052691	4.783128
255.447407	7881.410537	14.340877	-0.052639	4.780779
255.477568	7873.462063	14.345882	-0.052639	4.778437
255.483019	7865.410195	14.350887	-0.052635	4.776064
255.302172	7857.463679	14.355891	-0.052596	4.773722
255.117482	7849.312665	14.360896	-0.052557	4.771318
255.331991	7841.336832	14.365901	-0.052592	4.768963
255.237059	7833.394895	14.370906	-0.052569	4.766618
255.163577	7825.409630	14.375911	-0.052550	4.764259
255.228604	7817.409939	14.380915	-0.052557	4.761894
255.031744	7809.315108	14.385920	-0.052515	4.759501
254.929803	7801.414340	14.390925	-0.052491	4.757164
255.094511	7793.370799	14.395930	-0.052516	4.754782
254.768158	7785.304709	14.400935	-0.052450	4.752394
254.841643	7777.320895	14.405939	-0.052459	4.750028
254.674723	7769.317410	14.410944	-0.052423	4.747655
254.594759	7761.290503	14.415949	-0.052402	4.745274
254.709469	7753.340134	14.420954	-0.052419	4.742914
254.686576	7745.332379	14.425959	-0.052409	4.740537
254.696243	7737.378360	14.430963	-0.052406	4.738174
254.494120	7729.365347	14.435968	-0.052363	4.735792
254.334900	7721.340066	14.440973	-0.052328	4.733406
254.427376	7713.289785	14.445978	-0.052340	4.731011
254.303120	7705.334885	14.450983	-0.052312	4.728643
254.308412	7697.328597	14.455987	-0.052308	4.726259
254.268253	7689.298724	14.460992	-0.052295	4.723866
254.355069	7681.353598	14.465997	-0.052306	4.721497
254.338477	7673.304837	14.471002	-0.052298	4.719096
254.121839	7665.336986	14.476007	-0.052252	4.716719
254.129317	7657.319635	14.481011	-0.052248	4.714325
254.148201	7649.269884	14.486016	-0.052247	4.711920
254.031787	7641.252454	14.491021	-0.052220	4.709524
254.128834	7633.340935	14.496026	-0.052233	4.707157
254.049685	7625.268315	14.501031	-0.052213	4.704742
253.967674	7617.339572	14.506035	-0.052192	4.702369
253.907483	7609.292052	14.511040	-0.052176	4.699959
253.957864	7601.352541	14.516045	-0.052180	4.697579
253.905046	7593.301863	14.521050	-0.052165	4.695166
253.720678	7585.290948	14.526055	-0.052126	4.692763
253.825549	7577.254769	14.531059	-0.052140	4.690351
253.714954	7569.251571	14.536064	-0.052114	4.687948
253.623000	7561.267179	14.541069	-0.052092	4.685549
253.642997	7553.295839	14.546074	-0.052091	4.683153
253.570015	7545.287612	14.551079	-0.052072	4.680745
253.651854	7537.349682	14.556083	-0.052082	4.678356
253.536415	7529.293515	14.561088	-0.052055	4.675931
253.316906	7521.202753	14.566093	-0.052009	4.673494
253.399502	7513.168413	14.571098	-0.052019	4.671073
253.317462	7505.188227	14.576103	-0.051999	4.668667
253.333441	7497.219841	14.581107	-0.051997	4.666263
253.252820	7489.215890	14.586112	-0.051976	4.663847
253.258825	7481.222650	14.591117	-0.051972	4.661433
253.230809	7473.241700	14.596122	-0.051962	4.659022
253.260485	7465.214505	14.601127	-0.051962	4.656595
253.276075	7457.245106	14.606131	-0.051960	4.654185
253.232114	7449.231188	14.611136	-0.051947	4.651759
253.106060	7441.198568	14.616141	-0.051918	4.649327
252.892935	7433.245197	14.621146	-0.051873	4.646918
252.760502	7425.178841	14.626151	-0.051843	4.644473
252.874082	7417.311849	14.631155	-0.051859	4.642087
252.821655	7409.231485	14.636160	-0.051844	4.639636
252.614101	7401.250758	14.641165	-0.051800	4.637213
252.679464	7393.192522	14.646170	-0.051807	4.634765
252.723946	7385.164171	14.651175	-0.051810	4.632326
252.658588	7377.193287	14.656179	-0.051793	4.629902
252.402494	7369.165883	14.661184	-0.051740	4.627460
252.496933	7361.168750	14.666189	-0.051753	4.625026
252.517301	7353.218797	14.671194	-0.051751	4.622605
252.239902	7345.170445	14.676199	-0.051694	4.620152
252.395670	7337.225895	14.681203	-0.051718	4.617730
252.442748	7329.227131	14.686208	-0.051722	4.615290
252.458128	7321.152821	14.691213	-0.051720	4.612826
252.398792	7313.138050	14.696218	-0.051703	4.610379
252.318466	7305.169462	14.701223	-0.051683	4.607944
252.265462	7297.179579	14.706227	-0.051668	4.605502
252.165030	7289.191966	14.711232	-0.051644	4.603059
252.325280	7281.186931	14.716237	-0.051669	4.600609
252.083610	7273.192747	14.721242	-0.051619	4.598162
251.823626	7265.154042	14.726247	-0.051565	4.595699
251.795597	7257.131584	14.731251	-0.051555	4.593240
251.655078	7249.107546	14.736256	-0.051523	4.590780
251.594108	7241.140604	14.741261	-0.051507	4.588335
251.578878	7233.151402	14.746266	-0.051499	4.585882
251.598558	7225.151160	14.751271	-0.051497	4.583425
251.699411	7217.110307	14.756275	-0.051511	4.580954
251.602758	7209.143349	14.761280	-0.051488	4.578504
251.615792	7201.125583	14.766285	-0.051485	4.576037
251.608034	7193.142630	14.771290	-0.051478	4.573580
251.668658	7185.068483	14.776295	-0.051484	4.571093
251.381507	7177.141777	14.781299	-0.051426	4.568650
251.237102	7169.127777	14.786304	-0.051394	4.566179
251.345033	7161.145494	14.791309	-0.051409	4.563717
251.349728	7153.175000	14.796314	-0.051404	4.561257
251.074582	7145.096851	14.801319	-0.051348	4.558762
251.067654	7137.220997	14.806323	-0.051342	4.556328
250.874915	7129.161464	14.811328	-0.051300	4.553836
250.895146	7121.071060	14.816333	-0.051299	4.551334
250.764083	7113.099843	14.821338	-0.051269	4.548866
250.669154	7105.089477	14.826343	-0.051246	4.546386
250.733492	7097.084656	14.831347	-0.051253	4.543905
250.678272	7089.136224	14.836352	-0.051238	4.541441
250.807741	7081.130662	14.841357	-0.051257	4.538958
250.613802	7073.159585	14.846362	-0.051216	4.536484
250.588632	7065.076281	14.851367	-0.051206	4.533974
250.785925	7057.146703	14.856371	-0.051237	4.531511
250.641630	7049.131296	14.861376	-0.051205	4.529019
250.586705	7041.113726	14.866381	-0.051190	4.526525
250.653936	7033.142860	14.871386	-0.051197	4.524045
250.499544	7025.137873	14.876391	-0.051163	4.521552
250.503164	7017.130173	14.881395	-0.051159	4.519057
250.472287	7009.128169	14.886400	-0.051148	4.516562
250.559575	7001.115663	14.891405	-0.051159	4.514063
250.517817	6993.033601	14.896410	-0.051146	4.511541
250.403856	6985.026652	14.901415	-0.051119	4.509041
250.409960	6977.050154	14.906419	-0.051115	4.506549
250.155025	6969.073346	14.911424	-0.051063	4.504055
250.204152	6961.095377	14.916429	-0.051067	4.501560
250.222181	6953.080213	14.921434	-0.051065	4.499051
250.066757	6945.063150	14.926439	-0.051031	4.496541
249.961283	6937.079052	14.931443	-0.051006	4.494039
249.930216	6929.048949	14.936448	-0.050995	4.491522
250.020838	6921.027148	14.941453	-0.051007	4.489006
249.861596	6913.082935	14.946458	-0.050972	4.486512
249.739557	6905.033488	14.951463	-0.050944	4.483985
250.000835	6897.093925	14.956467	-0.050987	4.481491
249.797683	6889.075244	14.961472	-0.050944	4.478970
249.627894	6881.075690	14.966477	-0.050908	4.476453
249.776643	6873.063325	14.971482	-0.050930	4.473932
249.595635	6864.967924	14.976487	-0.050891	4.471382
249.672089	6857.026847	14.981491	-0.050900	4.468881
249.423580	6849.025641	14.986496	-0.050849	4.466357
249.411354	6841.039145	14.991501	-0.050841	4.463838
249.397847	6833.044330	14.996506	-0.050834	4.461315
249.293973	6825.037358	15.001511	-0.050809	4.458786
249.249209	6817.043139	15.006515	-0.050796	4.456260
249.015414	6808.984766	15.011520	-0.050747	4.453712
249.225923	6800.976756	15.016525	-0.050781	4.451179
249.250604	6793.021979	15.021530	-0.050780	4.448662
248.961519	6784.989090	15.026535	-0.050721	4.446117
249.098612	6777.036019	15.031539	-0.050742	4.443597
248.881493	6769.055772	15.036544	-0.050696	4.441066
248.984214	6761.012818	15.041549	-0.050710	4.438515
248.928453	6753.054340	15.046554	-0.050694	4.435989
248.876165	6744.994239	15.051559	-0.050679	4.433429
248.809868	6736.977328	15.056563	-0.050662	4.430881
248.677758	6728.938530	15.061568	-0.050632	4.428325
248.706925	6720.952102	15.066573	-0.050632	4.425784
248.672980	6713.018258	15.071578	-0.050621	4.423258
248.685832	6704.962833	15.076583	-0.050618	4.420692
248.696729	6697.009072	15.081587	-0.050615	4.418158
248.450544	6688.987506	15.086592	-0.050564	4.415599
248.515686	6680.947240	15.091597	-0.050571	4.413034
248.490942	6672.974646	15.096602	-0.050561	4.410488
248.381567	6664.952336	15.101607	-0.050535	4.407925
248.400848	6656.983434	15.106611	-0.050534	4.405378
248.172713	6649.014419	15.111616	-0.050486	4.402828
248.091155	6640.963804	15.116621	-0.050466	4.400252
248.202154	6633.025834	15.121626	-0.050481	4.397711
248.009039	6624.968988	15.126631	-0.050440	4.395129
247.998243	6616.978088	15.131635	-0.050433	4.392567
247.956218	6608.957374	15.136640	-0.050420	4.389994
248.132079	6600.938530	15.141645	-0.050448	4.387422
247.994758	6592.981405	15.146650	-0.050417	4.384866
247.704662	6585.005499	15.151655	-0.050358	4.382301
247.961514	6576.990476	15.156659	-0.050400	4.379726
247.945168	6569.020986	15.161664	-0.050392	4.377162
247.730752	6560.987128	15.166669	-0.050347	4.374575
247.455113	6553.004810	15.171674	-0.050290	4.372002
247.579914	6544.955807	15.176679	-0.050309	4.369409
247.542409	6537.013371	15.181683	-0.050296	4.366848
247.713934	6528.945825	15.186688	-0.050323	4.364246
247.389697	6521.038686	15.191693	-0.050258	4.361691
247.414046	6513.058914	15.196698	-0.050257	4.359114
247.382752	6505.003855	15.201703	-0.050246	4.356510
247.474114	6496.980119	15.206707	-0.050258	4.353916
247.348445	6488.882596	15.211712	-0.050229	4.351294
247.420967	6480.912221	15.216717	-0.050237	4.348714
247.501081	6472.935801	15.221722	-0.050247	4.346130
247.410723	6464.936851	15.226727	-0.050225	4.343537
247.349200	6456.955585	15.231731	-0.050209	4.340947
246.911668	6448.962105	15.236736	-0.050122	4.338350
246.974623	6440.940758	15.241741	-0.050128	4.335745
247.170314	6432.959757	15.246746	-0.050160	4.333153
246.793109	6424.916306	15.251751	-0.050084	4.330535
246.914937	6416.945542	15.256755	-0.050102	4.327942
246.962222	6408.939947	15.261760	-0.050105	4.325336
246.753905	6400.952560	15.266765	-0.050061	4.322733
246.725853	6392.988982	15.271770	-0.050051	4.320137
246.685590	6385.011348	15.276775	-0.050038	4.317535
246.642332	6376.968802	15.281779	-0.050025	4.314910
246.518909	6368.948327	15.286784	-0.049997	4.312290
246.455379	6360.926608	15.291789	-0.049980	4.309668
246.491858	6352.961857	15.296794	-0.049982	4.307064
246.507618	6344.921316	15.301799	-0.049979	4.304434
246.422893	6336.959608	15.306803	-0.049958	4.301827
246.497849	6328.915058	15.311808	-0.049967	4.299193
246.196114	6320.948393	15.316813	-0.049906	4.296579
246.194500	6312.924139	15.321818	-0.049900	4.293948
246.331045	6304.888078	15.326823	-0.049920	4.291312
246.254600	6296.925904	15.331827	-0.049901	4.288697
246.246318	6288.927964	15.336832	-0.049894	4.286069
245.914929	6280.923185	15.341837	-0.049827	4.283435
245.973758	6272.927747	15.346842	-0.049833	4.280805
245.757883	6264.929098	15.351847	-0.049788	4.278171
245.751245	6256.940474	15.356851	-0.049781	4.275539
245.920467	6248.909573	15.361856	-0.049808	4.272894
245.996249	6240.831150	15.366861	-0.049817	4.270231
245.840607	6232.943581	15.371866	-0.049783	4.267627
245.853237	6224.861686	15.376871	-0.049780	4.264958
245.868474	6216.933092	15.381875	-0.049777	4.262339
245.626946	6208.905866	15.386880	-0.049727	4.259683
245.519546	6200.940479	15.391885	-0.049702	4.257047
245.681668	6192.939676	15.396890	-0.049727	4.254400
245.427813	6184.863891	15.401895	-0.049675	4.251723
245.555095	6176.869329	15.406899	-0.049693	4.249075
245.422181	6168.903001	15.411904	-0.049663	4.246432
245.245181	6160.897793	15.416909	-0.049625	4.243774
245.183558	6152.960197	15.421914	-0.049608	4.241137
245.113760	6144.925413	15.426919	-0.049590	4.238467
245.196132	6136.940160	15.431923	-0.049600	4.235813
245.110495	6128.939429	15.436928	-0.049579	4.233151
245.028157	6120.842419	15.441933	-0.049559	4.230454
245.198449	6112.932457	15.446938	-0.049585	4.227821
244.994390	6104.903595	15.451943	-0.049542	4.225143
244.985641	6096.941475	15.456947	-0.049535	4.222488
245.122760	6088.913605	15.461952	-0.049556	4.219810
244.969828	6080.940653	15.466957	-0.049522	4.217146
244.709286	6072.963934	15.471962	-0.049468	4.214478
244.554834	6064.923800	15.476967	-0.049434	4.211788
244.968457	6056.908720	15.481971	-0.049506	4.209111
244.796484	6048.956782	15.486976	-0.049469	4.206447
244.731832	6040.948857	15.491981	-0.049452	4.203763
244.692829	6032.962966	15.496986	-0.049439	4.201086
244.559054	6024.943306	15.501991	-0.049409	4.198394
244.538995	6016.949420	15.506995	-0.049400	4.195711
244.305210	6008.857834	15.512000	-0.049352	4.192991
244.548809	6000.782279	15.517005	-0.049392	4.190279
244.533972	5992.838066	15.522010	-0.049384	4.187607
244.237296	5984.885834	15.527015	-0.049323	4.184928
244.463993	5976.930987	15.532019	-0.049360	4.182252
244.347120	5968.895186	15.537024	-0.049333	4.179543
244.198681	5960.918455	15.542029	-0.049301	4.176852
244.178225	5952.963028	15.547034	-0.049292	4.174168
244.096336	5944.879820	15.552039	-0.049271	4.171438
243.976235	5936.935339	15.557043	-0.049244	4.168752
243.897828	5928.897682	15.562048	-0.049224	4.166034
243.784807	5920.876638	15.567053	-0.049198	4.163320
243.789191	5912.949985	15.572058	-0.049193	4.160637
243.597706	5904.951343	15.577063	-0.049153	4.157925
243.801562	5896.898277	15.582067	-0.049185	4.155198
243.759256	5888.875556	15.587072	-0.049172	4.152477
243.556876	5880.853606	15.592077	-0.049129	4.149752
243.508814	5872.895915	15.597082	-0.049115	4.147049
243.657776	5864.867586	15.602087	-0.049138	4.144322
243.549435	5856.931655	15.607091	-0.049112	4.141623
243.554131	5848.885926	15.612096	-0.049108	4.138885
243.289577	5840.910207	15.617101	-0.049054	4.136166
243.496178	5832.896245	15.622106	-0.049087	4.133438
243.328040	5824.866337	15.627111	-0.049050	4.130698
243.406663	5816.896848	15.632115	-0.049060	4.127980
243.109203	5808.891552	15.637120	-0.048999	4.125243
243.036861	5800.902567	15.642125	-0.048981	4.122513
243.084376	5792.913549	15.647130	-0.048984	4.119783
243.113352	5784.936893	15.652135	-0.048985	4.117054
243.121060	5776.898849	15.657139	-0.048981	4.114303
242.984520	5768.860695	15.662144	-0.048950	4.111548
242.914031	5760.836414	15.667149	-0.048932	4.108796
242.832700	5752.878010	15.672154	-0.048912	4.106065
242.538601	5744.893082	15.677159	-0.048852	4.103321
242.759514	5736.876537	15.682163	-0.048888	4.100570
242.888082	5728.918803	15.687168	-0.048906	4.097837
242.845851	5720.874967	15.692173	-0.048893	4.095070
242.632589	5712.900406	15.697178	-0.048848	4.092323
242.528827	5704.846342	15.702183	-0.048824	4.089548
242.486532	5696.940268	15.707187	-0.048811	4.086822
242.415371	5688.935656	15.712192	-0.048792	4.084061
242.410586	5680.926615	15.717197	-0.048786	4.081297
242.427299	5672.965529	15.722202	-0.048784	4.078548
242.197655	5664.993530	15.727207	-0.048736	4.075790
242.163107	5656.962283	15.732211	-0.048725	4.073013
242.173615	5648.887806	15.737216	-0.048722	4.070219
241.966876	5640.906155	15.742221	-0.048678	4.067452
242.149186	5632.915877	15.747226	-0.048707	4.064686
242.133855	5624.940912	15.752231	-0.048699	4.061920
241.861280	5616.951458	15.757235	-0.048643	4.059144
242.041217	5608.973041	15.762240	-0.048671	4.056377
242.091278	5600.922792	15.767245	-0.048675	4.053580
241.928602	5592.896886	15.772250	-0.048640	4.050787
241.768772	5584.918629	15.777255	-0.048605	4.048009
241.676352	5576.925140	15.782259	-0.048582	4.045224
241.871068	5568.945585	15.787264	-0.048613	4.042447
241.721157	5560.925302	15.792269	-0.048580	4.039649
241.704180	5552.986339	15.797274	-0.048572	4.036878
241.528887	5544.905026	15.802279	-0.048534	4.034054
241.452124	5536.839476	15.807283	-0.048515	4.031235
241.432847	5528.891362	15.812288	-0.048506	4.028456
241.259004	5520.882360	15.817293	-0.048468	4.025651
241.337123	5512.907177	15.822298	-0.048478	4.022860
241.208384	5504.908323	15.827303	-0.048449	4.020056
241.169888	5496.942270	15.832307	-0.048436	4.017262
241.260930	5488.919978	15.837312	-0.048448	4.014449
241.214240	5480.892545	15.842317	-0.048434	4.011630
241.120562	5472.928850	15.847322	-0.048411	4.008830
241.097313	5464.895691	15.852327	-0.048402	4.006005
241.065784	5456.907618	15.857331	-0.048391	4.003194
240.929989	5448.926371	15.862336	-0.048360	4.000382
240.871232	5440.933111	15.867341	-0.048344	3.997565
241.097623	5432.923595	15.872346	-0.048381	3.994744
240.948179	5424.882110	15.877351	-0.048348	3.991904
240.738012	5416.876624	15.882355	-0.048304	3.989074
240.764754	5408.902130	15.887360	-0.048304	3.986257
240.642610	5400.897845	15.892365	-0.048276	3.983425
240.615172	5392.931038	15.897370	-0.048266	3.980605
240.702663	5384.920425	15.902375	-0.048277	3.977770
240.703841	5376.914282	15.907379	-0.048272	3.974933
240.449469	5368.933893	15.912384	-0.048219	3.972099
240.519468	5360.898147	15.917389	-0.048227	3.969249
240.679309	5352.957894	15.922394	-0.048252	3.966432
240.241772	5344.950884	15.927399	-0.048165	3.963579
240.268404	5336.985393	15.932403	-0.048165	3.960747
240.262849	5329.031537	15.937408	-0.048159	3.957916
240.153511	5320.976252	15.942413	-0.048133	3.955045
240.158075	5312.960721	15.947418	-0.048129	3.952188
239.961918	5304.904812	15.952423	-0.048087	3.949312
240.018530	5296.929007	15.957427	-0.048092	3.946466
239.934531	5288.954516	15.962432	-0.048071	3.943616
239.776560	5280.946711	15.967437	-0.048037	3.940751
239.896714	5273.005139	15.972442	-0.048054	3.937913
239.764751	5264.984183	15.977447	-0.048024	3.935039
239.774288	5256.992552	15.982451	-0.048021	3.932177
239.859273	5248.979443	15.987456	-0.048032	3.929306
239.672723	5240.978041	15.992461	-0.047992	3.926432
239.767999	5233.010896	15.997466	-0.048004	3.923573
239.557556	5225.017299	16.002471	-0.047960	3.920698
239.630198	5217.012603	16.007475	-0.047968	3.917821
239.404319	5209.035137	16.012480	-0.047921	3.914947
239.383585	5200.956867	16.017485	-0.047912	3.912038
239.683380	5192.963338	16.022490	-0.047963	3.909163
239.380551	5184.979980	16.027495	-0.047901	3.906279
239.423501	5176.985527	16.032499	-0.047904	3.903394
239.422491	5168.990625	16.037504	-0.047898	3.900507
239.325046	5160.995479	16.042509	-0.047875	3.897616
239.214457	5153.013046	16.047514	-0.047849	3.894727
239.152792	5144.967613	16.052519	-0.047833	3.891814
239.325427	5136.979577	16.057523	-0.047860	3.888924
239.085807	5129.013316	16.062528	-0.047810	3.886031
238.671526	5121.001338	16.067533	-0.047728	3.883117
239.118470	5113.017324	16.072538	-0.047806	3.880227
238.920627	5105.046260	16.077543	-0.047764	3.877328
238.876772	5096.994826	16.082547	-0.047750	3.874399
238.956534	5088.766976	16.087552	-0.047760	3.871407
238.846114	5080.841199	16.092557	-0.047734	3.868519
238.635151	5072.906327	16.097562	-0.047690	3.865623
238.653468	5064.943549	16.102567	-0.047688	3.862720
238.842821	5056.954272	16.107571	-0.047718	3.859808
238.607184	5049.032832	16.112576	-0.047669	3.856910
238.389245	5040.995228	16.117581	-0.047623	3.853968
238.342882	5033.008940	16.122586	-0.047609	3.851046
238.317958	5024.960196	16.127591	-0.047599	3.848099
238.181557	5016.964758	16.132595	-0.047569	3.845167
238.258964	5009.035842	16.137600	-0.047578	3.842262
238.090220	5001.014477	16.142605	-0.047542	3.839315
238.130961	4993.097156	16.147610	-0.047544	3.836409
238.072083	4985.048792	16.152615	-0.047528	3.833450
238.163376	4976.992191	16.157619	-0.047540	3.830489
237.959452	4969.059543	16.162624	-0.047497	3.827566
237.775796	4961.009876	16.167629	-0.047457	3.824597
238.001524	4953.099656	16.172634	-0.047494	3.821686
237.879181	4945.062309	16.177639	-0.047466	3.818719
237.753958	4937.077085	16.182643	-0.047438	3.815768
237.838601	4929.071559	16.187648	-0.047448	3.812812
237.823789	4921.023140	16.192653	-0.047440	3.809836
237.627774	4913.106307	16.197658	-0.047399	3.806902
237.677023	4905.078481	16.202663	-0.047403	3.803930
237.507023	4897.154012	16.207667	-0.047366	3.800990
237.725090	4889.090016	16.212672	-0.047401	3.798003
237.437651	4881.095825	16.217677	-0.047342	3.795030
237.464357	4873.064173	16.222682	-0.047342	3.792047
237.517556	4865.038097	16.227687	-0.047347	3.789064
237.402928	4857.064423	16.232691	-0.047320	3.786095
237.132695	4849.102200	16.237696	-0.047265	3.783124
236.980757	4841.084807	16.242701	-0.047231	3.780132
237.143116	4833.120966	16.247706	-0.047256	3.777166
236.920433	4825.076267	16.252711	-0.047210	3.774158
237.015868	4817.071392	16.257715	-0.047222	3.771170
237.052462	4809.081421	16.262720	-0.047224	3.768184
237.156978	4801.049414	16.267725	-0.047238	3.765181
237.152776	4793.150459	16.272730	-0.047232	3.762223
237.131693	4785.097201	16.277735	-0.047223	3.759205
236.948664	4777.137807	16.282739	-0.047184	3.756216
236.783397	4769.118883	16.287744	-0.047148	3.753202
236.639421	4761.079402	16.292749	-0.047116	3.750179
236.649713	4753.119044	16.297754	-0.047113	3.747186
236.541752	4745.089493	16.302759	-0.047088	3.744163
236.576543	4737.127978	16.307763	-0.047089	3.741165
236.523059	4729.140292	16.312768	-0.047074	3.738154
236.436433	4721.115654	16.317773	-0.047052	3.735125
236.292613	4713.151619	16.322778	-0.047020	3.732116
236.285106	4705.134211	16.327783	-0.047014	3.729087
236.498763	4697.110076	16.332787	-0.047048	3.726058
236.129530	4689.184021	16.337792	-0.046975	3.723050
236.270320	4681.177493	16.342797	-0.046996	3.720021
236.460266	4673.206387	16.347802	-0.047026	3.717005
236.216761	4665.174981	16.352807	-0.046975	3.713953
236.286825	4657.068379	16.357811	-0.046983	3.710877
236.042043	4649.140007	16.362816	-0.046932	3.707858
235.869481	4641.109283	16.367821	-0.046895	3.704800
235.921911	4633.175565	16.372826	-0.046900	3.701782
235.806160	4625.215872	16.377831	-0.046873	3.698748
235.676154	4617.204759	16.382835	-0.046844	3.695691
235.683594	4609.213384	16.387840	-0.046840	3.692642
235.817411	4601.155708	16.392845	-0.046859	3.689569
235.792152	4593.232811	16.397850	-0.046850	3.686540
235.407382	4585.239932	16.402855	-0.046773	3.683474
235.374531	4577.232914	16.407859	-0.046761	3.680408
235.620037	4569.233562	16.412864	-0.046802	3.677350
235.394321	4561.247070	16.417869	-0.046755	3.674282
235.717721	4553.215857	16.422874	-0.046810	3.671208
235.563024	4545.230730	16.427879	-0.046776	3.668137
235.500466	4537.223413	16.432883	-0.046759	3.665058
235.396908	4529.260515	16.437888	-0.046735	3.661991
235.308143	4521.218232	16.442893	-0.046713	3.658893
235.260036	4513.288553	16.447898	-0.046699	3.655835
235.352165	4505.240254	16.452903	-0.046711	3.652734
235.159996	4497.219841	16.457907	-0.046670	3.649633
235.095172	4489.298559	16.462912	-0.046652	3.646571
234.863881	4481.288089	16.467917	-0.046604	3.643467
234.860449	4473.281721	16.472922	-0.046598	3.640368
234.991950	4465.324396	16.477927	-0.046618	3.637290
234.823507	4457.306840	16.482931	-0.046581	3.634177
234.708812	4449.269971	16.487936	-0.046555	3.631056
234.655312	4441.249457	16.492941	-0.046539	3.627940
234.854301	4433.254315	16.497946	-0.046571	3.624838
234.650583	4425.307849	16.502951	-0.046528	3.621741
234.722478	4417.247075	16.507955	-0.046536	3.618605
234.688384	4409.325677	16.512960	-0.046525	3.615517
234.502656	4401.306580	16.517965	-0.046485	3.612384
234.336855	4393.297911	16.522970	-0.046449	3.609254
234.339484	4385.340992	16.527975	-0.046444	3.606145
234.493335	4377.330665	16.532979	-0.046468	3.603017
234.451029	4369.360407	16.537984	-0.046455	3.599897
234.169665	4361.389543	16.542989	-0.046397	3.596767
234.119702	4353.376463	16.547994	-0.046383	3.593624
234.107403	4345.351003	16.552999	-0.046375	3.590474
234.043918	4337.368877	16.558003	-0.046358	3.587338
233.936004	4329.370791	16.563008	-0.046333	3.584191
233.820363	4321.394623	16.568013	-0.046306	3.581049
233.796963	4313.419577	16.573018	-0.046297	3.577908
233.760715	4305.417651	16.578023	-0.046285	3.574753
233.974622	4297.389441	16.583027	-0.046320	3.571593
233.933730	4289.389347	16.588032	-0.046307	3.568433
233.817475	4281.394021	16.593037	-0.046280	3.565270
234.026384	4273.431527	16.598042	-0.046314	3.562127
233.783254	4265.435361	16.603047	-0.046263	3.558954
233.675730	4257.467873	16.608051	-0.046238	3.555794
233.581974	4249.369580	16.613056	-0.046215	3.552580
233.386873	4241.341263	16.618061	-0.046174	3.549387
233.432436	4233.378436	16.623066	-0.046177	3.546225
233.159282	4225.382268	16.628071	-0.046121	3.543037
233.262069	4217.402771	16.633075	-0.046135	3.539864
233.401656	4209.447979	16.638080	-0.046156	3.536699
233.041548	4201.444909	16.643085	-0.046084	3.533497
232.942529	4193.427901	16.648090	-0.046060	3.530295
232.955523	4185.429233	16.653095	-0.046057	3.527100
232.936360	4177.441043	16.658099	-0.046049	3.523906
233.159891	4169.485236	16.663104	-0.046085	3.520729
233.090358	4161.494297	16.668109	-0.046067	3.517526
233.053093	4153.491072	16.673114	-0.046055	3.514316
233.119152	4145.458453	16.678119	-0.046062	3.511095
233.030543	4137.476195	16.683123	-0.046040	3.507886
232.997592	4129.497757	16.688128	-0.046029	3.504677
232.775301	4121.513413	16.693133	-0.045982	3.501458
232.788961	4113.563886	16.698138	-0.045980	3.498256
232.619300	4105.550001	16.703143	-0.045943	3.495021
232.576837	4097.542189	16.708147	-0.045930	3.491788
232.504126	4089.561184	16.713152	-0.045911	3.488562
232.318146	4081.561758	16.718157	-0.045871	3.485323
232.390798	4073.606569	16.723162	-0.045880	3.482106
232.348973	4065.596080	16.728167	-0.045867	3.478860
232.323505	4057.605654	16.733171	-0.045857	3.475620
232.301539	4049.580120	16.738176	-0.045848	3.472363
232.185667	4041.580353	16.743181	-0.045821	3.469110
232.287867	4033.566164	16.748186	-0.045835	3.465856
232.220060	4025.621355	16.753191	-0.045817	3.462621
232.146925	4017.611648	16.758195	-0.045798	3.459356
232.156894	4009.638846	16.763200	-0.045795	3.456106
231.855363	4001.629020	16.768205	-0.045733	3.452828
231.869095	3993.591585	16.773210	-0.045731	3.449545
231.728961	3985.652092	16.778215	-0.045700	3.446294
231.704930	3977.655085	16.783219	-0.045690	3.443021
231.832397	3969.660247	16.788224	-0.045708	3.439750
231.526228	3961.710555	16.793229	-0.045646	3.436481
231.618373	3953.695004	16.798234	-0.045658	3.433194
231.699017	3945.627261	16.803239	-0.045668	3.429883
231.519167	3937.665289	16.808243	-0.045629	3.426603
231.546873	3929.662124	16.813248	-0.045629	3.423310
231.368917	3921.697989	16.818253	-0.045591	3.420022
231.420432	3913.718862	16.823258	-0.045595	3.416734
231.329254	3905.722169	16.828263	-0.045573	3.413430
231.192951	3897.721151	16.833267	-0.045543	3.410119
231.322475	3889.722460	16.838272	-0.045562	3.406815
231.295781	3881.730174	16.843277	-0.045552	3.403506
231.301147	3873.770110	16.848282	-0.045547	3.400207
230.990258	3865.821689	16.853287	-0.045484	3.396900
231.002151	3857.770642	16.858291	-0.045481	3.393557
231.053199	3849.700206	16.863296	-0.045486	3.390205
230.805790	3841.736410	16.868301	-0.045434	3.386883
230.794190	3833.750874	16.873306	-0.045427	3.383557
230.693689	3825.797949	16.878311	-0.045403	3.380239
230.850114	3817.815365	16.883315	-0.045427	3.376913
230.966930	3809.802107	16.888320	-0.045444	3.373571
230.698488	3801.799748	16.893325	-0.045389	3.370215
230.513212	3793.861011	16.898330	-0.045349	3.366886
230.436791	3785.847147	16.903335	-0.045330	3.363526
230.441268	3777.849267	16.908339	-0.045325	3.360173
230.329385	3769.907301	16.913344	-0.045299	3.356835
230.635002	3761.837020	16.918349	-0.045351	3.353455
230.630402	3753.834940	16.923354	-0.045345	3.350089
230.473060	3745.871931	16.928359	-0.045310	3.346731
230.421551	3737.866340	16.933363	-0.045296	3.343355
230.416031	3729.909980	16.938368	-0.045289	3.339998
230.248710	3721.938793	16.943373	-0.045253	3.336626
230.236503	3713.931925	16.948378	-0.045246	3.333241
229.976453	3705.926893	16.953383	-0.045192	3.329844
230.045765	3697.945437	16.958387	-0.045200	3.326465
229.840896	3689.991038	16.963392	-0.045156	3.323085
230.037916	3681.952048	16.968397	-0.045188	3.319680
229.793451	3674.015317	16.973402	-0.045137	3.316299
229.828236	3665.973296	16.978407	-0.045139	3.312879
229.662093	3657.957401	16.983411	-0.045102	3.309460
229.856101	3649.985920	16.988416	-0.045133	3.306070
229.663398	3642.005811	16.993421	-0.045092	3.302658
229.808498	3634.033085	16.998426	-0.045114	3.299258
229.851354	3626.042633	17.003431	-0.045117	3.295844
229.686889	3618.033846	17.008435	-0.045081	3.292410
229.644244	3610.063329	17.013440	-0.045068	3.288994
229.333085	3602.072205	17.018445	-0.045005	3.285554
229.281643	3594.114840	17.023450	-0.044990	3.282136
229.292431	3586.110064	17.028455	-0.044987	3.278696
229.152018	3578.115798	17.033459	-0.044956	3.275251
229.224013	3570.108532	17.038464	-0.044964	3.271806
229.169652	3562.087165	17.043469	-0.044949	3.268345
228.870019	3554.126355	17.048474	-0.044888	3.264898
228.810119	3546.152894	17.053479	-0.044871	3.261450
228.848753	3538.163712	17.058483	-0.044873	3.257996
229.006667	3530.152572	17.063488	-0.044898	3.254534
228.974572	3522.139299	17.068493	-0.044886	3.251060
228.844748	3514.181023	17.073498	-0.044857	3.247601
228.748377	3506.170728	17.078503	-0.044834	3.244118
228.553341	3498.221282	17.083507	-0.044793	3.240654
228.726221	3490.260619	17.088512	-0.044820	3.237196
228.610408	3482.236420	17.093517	-0.044793	3.233694
228.539797	3474.171696	17.098522	-0.044774	3.230173
228.416255	3466.200058	17.103527	-0.044746	3.226687
228.352323	3458.225809	17.108531	-0.044729	3.223198
228.167873	3450.245867	17.113536	-0.044690	3.219698
228.128432	3442.280294	17.118541	-0.044677	3.216206
228.220978	3434.262589	17.123546	-0.044689	3.212693
228.038727	3426.268176	17.128551	-0.044650	3.209176
227.980990	3418.297820	17.133555	-0.044634	3.205670
228.204544	3410.320195	17.138560	-0.044671	3.202168
227.964869	3402.339930	17.143565	-0.044621	3.198643
228.017609	3394.362693	17.148570	-0.044626	3.195127
228.073536	3386.343028	17.153575	-0.044631	3.191588
228.062566	3378.342153	17.158579	-0.044624	3.188051
227.934760	3370.376159	17.163584	-0.044595	3.184521
227.771141	3362.417568	17.168589	-0.044559	3.180988
227.726095	3354.414292	17.173594	-0.044545	3.177437
227.540234	3346.418088	17.178599	-0.044506	3.173879
227.588311	3338.395735	17.183603	-0.044509	3.170315
227.534486	3330.453240	17.188608	-0.044494	3.166778
227.511694	3322.446599	17.193613	-0.044485	3.163211
227.302147	3314.481129	17.198618	-0.044441	3.159649
227.382511	3306.523101	17.203623	-0.044450	3.156099
227.505322	3298.451186	17.208627	-0.044468	3.152497
227.320017	3290.483373	17.213632	-0.044428	3.148923
227.069310	3282.503940	17.218637	-0.044376	3.145337
227.029987	3274.564487	17.223642	-0.044364	3.141774
227.057920	3266.548936	17.228647	-0.044364	3.138176
227.180301	3258.532576	17.233651	-0.044382	3.134577
226.938392	3250.584169	17.238656	-0.044331	3.130989
227.032772	3242.551521	17.243661	-0.044344	3.127374
227.027097	3234.587131	17.248666	-0.044338	3.123781
226.844547	3226.648076	17.253671	-0.044298	3.120187
226.675543	3218.656189	17.258675	-0.044262	3.116566
226.531140	3210.678810	17.263680	-0.044230	3.112948
226.617074	3202.626524	17.268685	-0.044241	3.109303
226.596480	3194.658242	17.273690	-0.044232	3.105686
226.529518	3186.688789	17.278695	-0.044214	3.102063
226.320693	3178.696957	17.283699	-0.044170	3.098418
226.539454	3170.726457	17.288704	-0.044205	3.094799
226.391896	3162.707630	17.293709	-0.044173	3.091137
226.295887	3154.736247	17.298714	-0.044150	3.087494
226.184023	3146.758856	17.303719	-0.044124	3.083843
226.192910	3138.765776	17.308723	-0.044120	3.080187
226.236575	3130.829063	17.313728	-0.044123	3.076553
225.822716	3122.771347	17.318733	-0.044041	3.072839
226.006533	3114.739467	17.323738	-0.044070	3.069160
226.163715	3106.735457	17.328743	-0.044094	3.065488
225.871218	3098.809332	17.333747	-0.044034	3.061826
225.830183	3090.857587	17.338752	-0.044022	3.058160
225.776303	3082.848416	17.343757	-0.044006	3.054462
225.741732	3074.868601	17.348762	-0.043995	3.050774
225.679874	3066.893171	17.353767	-0.043978	3.047083
225.546002	3058.886361	17.358771	-0.043948	3.043369
225.554754	3050.946651	17.363776	-0.043945	3.039688
225.357671	3042.990835	17.368781	-0.043903	3.035986
225.529149	3034.951506	17.373786	-0.043929	3.032258
225.443094	3026.958156	17.378791	-0.043908	3.028534
225.216746	3018.979930	17.383795	-0.043861	3.024806
225.315510	3011.034563	17.388800	-0.043874	3.021105
225.355199	3003.013543	17.393805	-0.043876	3.017361
225.353976	2995.042110	17.398810	-0.043871	3.013633
225.203112	2987.039610	17.403815	-0.043838	3.009879
225.300343	2979.045704	17.408819	-0.043851	3.006136
225.289388	2971.107671	17.413824	-0.043843	3.002410
225.092287	2963.119484	17.418829	-0.043802	2.998646
224.940458	2955.160513	17.423834	-0.043768	2.994893
225.010209	2947.128518	17.428839	-0.043776	2.991112
224.760261	2939.149180	17.433843	-0.043724	2.987336
224.671412	2931.190673	17.438848	-0.043702	2.983572
224.681769	2923.181549	17.443853	-0.043699	2.979785
224.534111	2915.221212	17.448858	-0.043667	2.976008
224.431701	2907.230029	17.453863	-0.043642	2.972214
224.541826	2899.197421	17.458867	-0.043658	2.968406
224.594714	2891.237653	17.463872	-0.043662	2.964625
224.323952	2883.284132	17.468877	-0.043607	2.960825
224.461450	2875.319907	17.473882	-0.043627	2.957037
224.450767	2867.311847	17.478887	-0.043620	2.953215
224.252561	2859.317452	17.483891	-0.043578	2.949385
224.315042	2851.349011	17.488896	-0.043584	2.945575
224.336589	2843.346441	17.493901	-0.043583	2.941743
224.283203	2835.383246	17.498906	-0.043568	2.937920
223.979716	2827.423241	17.503911	-0.043506	2.934081
223.825329	2819.409552	17.508915	-0.043473	2.930219
223.941638	2811.443669	17.513920	-0.043489	2.926389
223.870410	2803.443329	17.518925	-0.043471	2.922527
223.820632	2795.497127	17.523930	-0.043456	2.918688
223.908974	2787.512684	17.528935	-0.043467	2.914832
223.622769	2779.427877	17.533939	-0.043409	2.910903
223.611564	2771.486656	17.538944	-0.043402	2.907052
223.611295	2763.482128	17.543949	-0.043396	2.903167
223.638672	2755.505799	17.548954	-0.043396	2.899291
223.601947	2747.572863	17.553959	-0.043384	2.895428
223.388458	2739.573491	17.558963	-0.043339	2.891518
223.470248	2731.612319	17.563968	-0.043350	2.887637
223.211195	2723.621879	17.568973	-0.043296	2.883718
223.248004	2715.652787	17.573978	-0.043298	2.879820
223.397236	2707.681902	17.578983	-0.043320	2.875922
223.191153	2699.699845	17.583987	-0.043277	2.871994
223.177762	2691.694513	17.588992	-0.043269	2.868060
223.120030	2683.715299	17.593997	-0.043253	2.864130
222.934108	2675.774154	17.599002	-0.043214	2.860207
222.893790	2667.804830	17.604007	-0.043201	2.856273
222.801638	2659.794268	17.609011	-0.043179	2.852310
222.994340	2651.799245	17.614016	-0.043209	2.848365
222.762494	2643.834956	17.619021	-0.043161	2.844406
222.562574	2635.918501	17.624026	-0.043119	2.840467
222.632309	2627.920945	17.629031	-0.043126	2.836497
222.599993	2619.896003	17.634035	-0.043115	2.832502
222.578574	2611.923735	17.639040	-0.043106	2.828529
222.499719	2603.909217	17.644045	-0.043086	2.824526
222.564306	2595.952750	17.649050	-0.043093	2.820554
222.601324	2587.983804	17.654055	-0.043095	2.816569
222.347515	2579.999742	17.659059	-0.043042	2.812553
222.301076	2572.027614	17.664064	-0.043029	2.808550
222.235556	2564.020650	17.669069	-0.043011	2.804523
222.250790	2556.092776	17.674074	-0.043009	2.800534
222.278074	2548.105459	17.679079	-0.043009	2.796511
222.025939	2540.129834	17.684083	-0.042957	2.792471
221.825780	2532.169119	17.689088	-0.042914	2.788436
221.897883	2524.161285	17.694093	-0.042922	2.784387
221.849075	2516.207440	17.699098	-0.042908	2.780352
221.576826	2508.274620	17.704103	-0.042852	2.776309
221.516913	2500.259980	17.709107	-0.042836	2.772231
221.654692	2492.264070	17.714112	-0.042856	2.768169
221.501445	2484.287603	17.719117	-0.042823	2.764093
221.508440	2476.326178	17.724122	-0.042819	2.760028
221.507581	2468.359098	17.729127	-0.042814	2.755953
221.551089	2460.291364	17.734131	-0.042816	2.751824
221.585911	2452.328581	17.739136	-0.042818	2.747742
221.278663	2444.368819	17.744141	-0.042755	2.743635
221.407369	2436.401711	17.749146	-0.042774	2.739544
221.300776	2428.464019	17.754151	-0.042749	2.735448
221.162154	2420.444735	17.759155	-0.042718	2.731302
221.147548	2412.486951	17.764160	-0.042710	2.727189
221.024640	2404.528760	17.769165	-0.042682	2.723062
220.946524	2396.576152	17.774170	-0.042663	2.718935
221.009592	2388.608579	17.779175	-0.042669	2.714803
220.941886	2380.597345	17.784179	-0.042651	2.710634
220.834787	2372.658312	17.789184	-0.042626	2.706493
220.697072	2364.678933	17.794189	-0.042596	2.702323
220.793276	2356.693976	17.799194	-0.042608	2.698158
220.654807	2348.731661	17.804199	-0.042577	2.693984
220.638192	2340.719435	17.809203	-0.042569	2.689785
220.642699	2332.768893	17.814208	-0.042565	2.685613
220.650708	2324.786949	17.819213	-0.042561	2.681418
220.374626	2316.848955	17.824218	-0.042505	2.677222
220.383140	2308.857658	17.829223	-0.042501	2.673009
220.318219	2300.866613	17.834227	-0.042484	2.668785
220.442291	2292.868779	17.839232	-0.042502	2.664563
220.200025	2284.932350	17.844237	-0.042451	2.660343
220.112770	2276.982659	17.849242	-0.042430	2.656119
220.351052	2268.951242	17.854247	-0.042469	2.651866
220.074141	2260.991892	17.859251	-0.042412	2.647611
220.055328	2253.027565	17.864256	-0.042404	2.643364
220.097489	2245.056285	17.869261	-0.042406	2.639110
219.997413	2237.131671	17.874266	-0.042383	2.634865
219.749273	2229.148184	17.879271	-0.042331	2.630571
219.674749	2221.153813	17.884275	-0.042312	2.626276
219.718038	2213.204705	17.889280	-0.042315	2.622006
219.676439	2205.230653	17.894285	-0.042302	2.617710
219.737927	2197.239276	17.899290	-0.042309	2.613405
219.634506	2189.267375	17.904295	-0.042284	2.609092
219.383239	2181.312990	17.909299	-0.042232	2.604771
219.401656	2173.366531	17.914304	-0.042230	2.600466
219.375884	2165.406555	17.919309	-0.042220	2.596143
219.268220	2157.288527	17.924314	-0.042195	2.591721
219.010674	2149.301686	17.929319	-0.042142	2.587353
219.176456	2141.329119	17.934323	-0.042168	2.583015
219.210208	2133.406407	17.939328	-0.042169	2.578687
219.003863	2125.469347	17.944333	-0.042125	2.574327
219.074732	2117.477073	17.949338	-0.042133	2.569950
219.058831	2109.530047	17.954343	-0.042125	2.565583
218.957559	2101.580420	17.959347	-0.042101	2.561201
218.838865	2093.653166	17.964352	-0.042074	2.556824
218.819709	2085.655753	17.969357	-0.042065	2.552407
218.883943	2077.672881	17.974362	-0.042072	2.547996
218.692965	2069.742999	17.979367	-0.042031	2.543588
218.617314	2061.778563	17.984371	-0.042012	2.539162
218.704688	2053.797723	17.989376	-0.042023	2.534731
218.589839	2045.816011	17.994381	-0.041997	2.530277
218.270902	2037.887665	17.999386	-0.041932	2.525831
218.364803	2029.928105	18.004391	-0.041944	2.521389
218.102172	2021.975898	18.009395	-0.041890	2.516917
218.227125	2013.995673	18.014400	-0.041909	2.512450
218.173416	2005.985946	18.019405	-0.041893	2.507945
218.096743	1998.014375	18.024410	-0.041874	2.503451
217.787568	1990.103764	18.029415	-0.041811	2.498968
217.915579	1982.099392	18.034419	-0.041830	2.494455
217.885086	1974.133526	18.039424	-0.041819	2.489944
217.853817	1966.176157	18.044429	-0.041808	2.485429
217.756117	1958.231453	18.049434	-0.041785	2.480909
217.975505	1950.261688	18.054439	-0.041820	2.476389
217.734814	1942.290756	18.059443	-0.041770	2.471827
217.764185	1934.324850	18.064448	-0.041771	2.467279
217.697486	1926.362719	18.069453	-0.041753	2.462718
217.472505	1918.431729	18.074458	-0.041706	2.458154
217.562551	1910.473241	18.079463	-0.041718	2.453589
217.586238	1902.462054	18.084467	-0.041717	2.448981
217.495725	1894.526103	18.089472	-0.041695	2.444398
217.204049	1886.612385	18.094477	-0.041636	2.439805
217.105657	1878.655668	18.099482	-0.041612	2.435193
217.064579	1870.607808	18.104487	-0.041599	2.430523
216.897335	1862.648211	18.109491	-0.041563	2.425886
216.960910	1854.685436	18.114496	-0.041570	2.421256
216.885480	1846.736480	18.119501	-0.041550	2.416615
217.034251	1838.747717	18.124506	-0.041573	2.411959
216.880614	1830.819009	18.129511	-0.041539	2.407305
216.798813	1822.860266	18.134515	-0.041519	2.402630
216.937333	1814.907318	18.139520	-0.041539	2.397967
216.639086	1806.977211	18.144525	-0.041479	2.393274
216.473986	1799.018872	18.149530	-0.041443	2.388565
216.734129	1791.029143	18.154535	-0.041486	2.383862
216.549086	1783.091269	18.159539	-0.041447	2.379146
216.342876	1775.164208	18.164544	-0.041403	2.374424
216.280579	1767.168394	18.169549	-0.041386	2.369664
216.416128	1759.199715	18.174554	-0.041406	2.364926
216.440096	1751.265350	18.179559	-0.041406	2.360190
216.020036	1743.358636	18.184563	-0.041322	2.355426
216.067330	1735.354257	18.189568	-0.041326	2.350631
215.995424	1727.375305	18.194573	-0.041307	2.345831
215.958618	1719.428162	18.199578	-0.041295	2.341044
215.908407	1711.489545	18.204583	-0.041281	2.336251
215.684247	1703.533631	18.209587	-0.041234	2.331424
215.703783	1695.574526	18.214592	-0.041232	2.326604
215.622731	1687.629938	18.219597	-0.041212	2.321775
215.545800	1679.683413	18.224602	-0.041193	2.316936
215.596736	1671.727342	18.229607	-0.041197	2.312090
215.486224	1663.749259	18.234611	-0.041171	2.307208
215.534516	1655.811433	18.239616	-0.041175	2.302353
215.454948	1647.854737	18.244621	-0.041155	2.297466
215.339998	1639.909481	18.249626	-0.041129	2.292572
215.313303	1631.955176	18.254631	-0.041119	2.287670
215.215272	1624.000236	18.259635	-0.041095	2.282751
215.230080	1616.078163	18.264640	-0.041093	2.277851
214.966535	1608.117559	18.269645	-0.041039	2.272892
214.960830	1600.098126	18.274650	-0.041032	2.267909
214.998828	1592.155851	18.279655	-0.041034	2.262966
214.835407	1584.219391	18.284659	-0.040999	2.257998
214.958518	1576.260141	18.289664	-0.041016	2.253031
215.020263	1568.277644	18.294669	-0.041023	2.248032
214.964329	1560.357303	18.299674	-0.041007	2.243051
214.939144	1552.446819	18.304679	-0.040997	2.238068
214.779998	1544.497827	18.309683	-0.040963	2.233037
214.722591	1536.549391	18.314688	-0.040947	2.228005
214.482416	1528.614318	18.319693	-0.040897	2.222953
214.517041	1520.666696	18.324698	-0.040898	2.217906
214.464623	1512.730024	18.329703	-0.040883	2.212847
214.321101	1504.774276	18.334707	-0.040851	2.207756
214.250340	1496.838890	18.339712	-0.040833	2.202673
214.262785	1488.892114	18.344717	-0.040830	2.197578
214.008282	1480.975290	18.349722	-0.040778	2.192467
214.017029	1472.992144	18.354727	-0.040774	2.187324
213.955608	1465.041561	18.359731	-0.040758	2.182184
213.960132	1457.104951	18.364736	-0.040753	2.177047
213.952905	1449.153399	18.369741	-0.040747	2.171887
213.766595	1441.225849	18.374746	-0.040707	2.166714
213.776597	1433.291995	18.379751	-0.040704	2.161543
213.669921	1425.355586	18.384755	-0.040679	2.156346
213.843382	1417.397374	18.389760	-0.040706	2.151149
213.656555	1409.460194	18.394765	-0.040666	2.145920
213.396555	1401.553441	18.399770	-0.040612	2.140690
213.536970	1393.605173	18.404775	-0.040633	2.135459
213.519599	1385.629174	18.409779	-0.040625	2.130181
213.395410	1377.722630	18.414784	-0.040597	2.124926
213.362367	1369.793036	18.419789	-0.040586	2.119651
213.236104	1361.868797	18.424794	-0.040557	2.114357
213.173028	1353.867146	18.429799	-0.040540	2.109005
213.226147	1345.908824	18.434803	-0.040545	2.103679
213.211229	1337.995541	18.439808	-0.040537	2.098364
213.176699	1330.060220	18.444813	-0.040525	2.093018
213.024803	1322.128039	18.449818	-0.040492	2.087649
212.820805	1314.235223	18.454823	-0.040449	2.082288
212.665688	1306.317605	18.459827	-0.040415	2.076901
212.766293	1298.358817	18.464832	-0.040428	2.071497
212.795584	1290.404594	18.469837	-0.040429	2.066075
212.718151	1282.496384	18.474842	-0.040409	2.060660
212.658818	1274.585658	18.479847	-0.040393	2.055230
212.445812	1266.646496	18.484851	-0.040348	2.049751
212.594904	1258.708353	18.489856	-0.040371	2.044294
212.560651	1250.794976	18.494861	-0.040359	2.038822
212.292402	1242.894765	18.499866	-0.040304	2.033320
212.334715	1234.924822	18.504871	-0.040307	2.027786
212.087885	1227.008944	18.509875	-0.040256	2.022245
212.042592	1219.091182	18.514880	-0.040242	2.016708
211.961811	1211.155256	18.519885	-0.040222	2.011140
211.916908	1203.223608	18.524890	-0.040208	2.005563
211.991863	1195.302674	18.529895	-0.040217	1.999990
211.791622	1187.410615	18.534899	-0.040175	1.994393
211.753726	1179.471380	18.539904	-0.040163	1.988765
211.731905	1171.539288	18.544909	-0.040154	1.983127
211.651572	1163.628838	18.549914	-0.040133	1.977482
211.510872	1155.727773	18.554919	-0.040102	1.971821
211.508178	1147.783832	18.559923	-0.040096	1.966128
211.476299	1139.880904	18.564928	-0.040085	1.960444
211.247884	1131.991844	18.569933	-0.040038	1.954733
211.207719	1124.008708	18.574938	-0.040025	1.948958
211.133519	1116.101214	18.579943	-0.040006	1.943216
210.954939	1108.184381	18.584947	-0.039968	1.937440
210.925208	1100.274203	18.589952	-0.039957	1.931667
210.985945	1092.325021	18.594957	-0.039963	1.925858
210.958658	1084.420038	18.599962	-0.039953	1.920054
210.977008	1076.529930	18.604967	-0.039951	1.914249
210.799006	1068.601380	18.609971	-0.039913	1.908376
210.707971	1060.709852	18.614976	-0.039891	1.902521
210.604644	1052.815987	18.619981	-0.039867	1.896646
210.666496	1044.866321	18.624986	-0.039873	1.890729
210.664159	1036.962265	18.629991	-0.039868	1.884821
210.440462	1029.095061	18.634995	-0.039821	1.878896
210.499250	1021.182604	18.640000	-0.039827	1.872951
210.362207	1013.258376	18.645005	-0.039796	1.866956
210.146553	1005.368409	18.650010	-0.039751	1.860958
210.195328	997.464782	18.655015	-0.039755	1.854961
210.024799	989.549479	18.660019	-0.039718	1.848910
210.141297	981.623286	18.665024	-0.039734	1.842864
209.974149	973.763699	18.670029	-0.039698	1.836816
209.913850	965.847848	18.675034	-0.039682	1.830718
209.994329	957.939529	18.680039	-0.039692	1.824621
209.909291	950.041010	18.685043	-0.039671	1.818492
209.768185	942.177210	18.690048	-0.039639	1.812363
209.613079	934.275329	18.695053	-0.039605	1.806181
209.564229	926.385742	18.700058	-0.039591	1.800001
209.552867	918.500577	18.705063	-0.039584	1.793807
209.483224	910.537560	18.710067	-0.039566	1.787523
209.672737	902.618847	18.715072	-0.039596	1.781284
209.329920	894.791617	18.720077	-0.039527	1.775030
209.144280	886.904567	18.725082	-0.039487	1.768726
209.357871	878.992864	18.730087	-0.039522	1.762429
209.199798	871.122732	18.735091	-0.039487	1.756096
209.058450	863.253119	18.740096	-0.039456	1.749743
208.769625	855.411920	18.745101	-0.039397	1.743371
208.770227	847.510259	18.750106	-0.039392	1.736963
208.644253	839.630954	18.755111	-0.039364	1.730534
208.531991	831.752338	18.760115	-0.039338	1.724083
208.532228	823.884053	18.765120	-0.039333	1.717630
208.458017	815.994730	18.770125	-0.039314	1.711127
208.471982	808.081545	18.775130	-0.039311	1.704590
208.494099	800.223089	18.780135	-0.039310	1.698074
208.409075	792.339426	18.785139	-0.039289	1.691499
208.486264	784.450343	18.790144	-0.039299	1.684914
208.534924	776.590913	18.795149	-0.039302	1.678325
208.198750	768.766878	18.800154	-0.039235	1.671688
208.145835	760.889984	18.805159	-0.039220	1.665018
207.978814	753.042608	18.810163	-0.039184	1.658331
207.953199	745.176168	18.815168	-0.039174	1.651620
207.857467	737.309173	18.820173	-0.039151	1.644871
207.559451	729.496627	18.825178	-0.039090	1.638113
207.713136	721.567176	18.830183	-0.039114	1.631289
207.456197	713.706165	18.835187	-0.039061	1.624438
207.405796	705.859400	18.840192	-0.039046	1.617600
207.462340	697.981621	18.845197	-0.039052	1.610720
207.344854	690.143657	18.850202	-0.039025	1.603822
207.300154	682.314704	18.855207	-0.039012	1.596911
206.893966	674.505315	18.860211	-0.038931	1.589937
207.010611	666.630761	18.865216	-0.038947	1.582948
207.169838	658.757067	18.870221	-0.038972	1.575936
206.819138	650.951735	18.875226	-0.038902	1.568879
206.665149	643.138455	18.880231	-0.038868	1.561813
207.095300	635.221557	18.885235	-0.038943	1.554705
206.786143	627.414552	18.890240	-0.038880	1.547557
206.571026	619.610911	18.895245	-0.038835	1.540392
206.595368	611.768218	18.900250	-0.038835	1.533193
206.440495	603.953071	18.905255	-0.038801	1.525959
206.389040	596.126491	18.910259	-0.038786	1.518695
206.306906	588.307887	18.915264	-0.038766	1.511399
206.095560	580.497216	18.920269	-0.038721	1.504056
205.993060	572.685214	18.925274	-0.038697	1.496692
206.090493	564.846705	18.930279	-0.038710	1.489297
206.225227	556.998685	18.935283	-0.038730	1.481862
206.110068	549.217868	18.940288	-0.038704	1.474415
205.858890	541.384177	18.945293	-0.038652	1.466857
205.602730	533.611246	18.950298	-0.038599	1.459319
205.781630	525.783046	18.955303	-0.038627	1.451756
205.427987	518.013997	18.960307	-0.038557	1.444127
205.717684	510.184408	18.965312	-0.038605	1.436501
205.572279	502.400092	18.970317	-0.038573	1.428809
205.192154	494.651912	18.975322	-0.038497	1.421072
205.333601	486.850793	18.980327	-0.038519	1.413327
205.158173	479.066270	18.985331	-0.038481	1.405502
205.187778	471.299090	18.990336	-0.038482	1.397686
204.813199	463.545909	18.995341	-0.038407	1.389771
204.815173	455.746259	19.000346	-0.038402	1.381828
204.759373	447.986046	19.005351	-0.038387	1.373869
204.721083	440.193502	19.010355	-0.038374	1.365833
204.524998	432.476045	19.015360	-0.038333	1.357801
204.377172	424.721094	19.020365	-0.038300	1.349690
204.283643	416.961757	19.025370	-0.038278	1.341534
204.310766	409.207577	19.030375	-0.038278	1.333356
204.297516	401.438887	19.035379	-0.038271	1.325104
204.204816	393.719830	19.040384	-0.038248	1.316840
203.966957	385.894421	19.045389	-0.038199	1.308383
203.961446	378.137605	19.050394	-0.038193	1.299987
203.889143	370.425409	19.055399	-0.038174	1.291573
203.662567	362.729576	19.060403	-0.038127	1.283093
203.599617	355.032525	19.065408	-0.038111	1.274586
203.539802	347.311693	19.070413	-0.038094	1.265996
203.423928	339.615446	19.075418	-0.038068	1.257364
203.142546	331.952949	19.080423	-0.038010	1.248679
203.184465	324.234198	19.085427	-0.038013	1.239931
203.230913	316.531379	19.090432	-0.038017	1.231140
203.043074	308.849867	19.095437	-0.037977	1.222265
202.872546	301.192182	19.100442	-0.037940	1.213355
202.884397	293.504906	19.105447	-0.037938	1.204382
202.828679	285.844877	19.110451	-0.037922	1.195359
202.569399	278.215064	19.115456	-0.037869	1.186263
202.497884	270.569821	19.120461	-0.037851	1.177116
202.240005	262.940295	19.125466	-0.037798	1.167878
202.086700	255.320647	19.130471	-0.037764	1.158600
201.967033	247.656776	19.135475	-0.037737	1.149200
201.824744	240.033597	19.140480	-0.037706	1.139768
201.835027	232.393894	19.145485	-0.037703	1.130269
201.510669	224.828126	19.150490	-0.037637	1.120710
201.342287	217.249896	19.155495	-0.037601	1.111087
200.772842	209.721963	19.160499	-0.037490	1.101356
200.567030	202.152682	19.165504	-0.037447	1.091566
200.440629	194.575012	19.170509	-0.037418	1.081693
199.920260	187.071416	19.175514	-0.037317	1.071738
199.536949	179.541099	19.180519	-0.037240	1.061685
199.115419	172.028321	19.185523	-0.037157	1.051550
198.839508	164.505548	19.190528	-0.037101	1.041338
198.382510	157.028942	19.195533	-0.037011	1.031044
197.993474	149.532653	19.200538	-0.036934	1.020635
197.889210	142.018705	19.205543	-0.036909	1.010163
197.183363	134.610585	19.210547	-0.036773	0.999583
196.805616	127.133635	19.215552	-0.036698	0.988872
196.334408	119.693865	19.220557	-0.036605	0.978075
195.813721	112.280950	19.225562	-0.036504	0.967183
195.583166	104.849879	19.230567	-0.036456	0.956215
195.176352	97.444011	19.235571	-0.036375	0.945111
194.788949	90.068793	19.240576	-0.036298	0.933926
194.053848	82.758884	19.245581	-0.036157	0.922612
193.559689	75.416648	19.250586	-0.036060	0.911173
193.312707	68.049531	19.255591	-0.036009	0.899617
192.939225	60.948240	19.260595	-0.035935	0.888298