Thu Mar 11 21:04:49 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.417919	0.100706	0.000000	0.000020	0.722241

0.492608	0.027784	0.005005	0.000006	0.722124
0.467214	0.008571	0.010010	0.000011	0.722077
0.329260	0.034154	0.015014	0.000037	0.722079
0.572495	-0.006826	0.020019	-0.000009	0.722084
0.470117	0.006940	0.025024	0.000010	0.722075
0.386058	0.026344	0.030029	0.000026	0.722084
0.505517	0.001880	0.035034	0.000004	0.722078
0.519756	-0.000669	0.040038	0.000001	0.722078
0.423202	0.019371	0.045043	0.000019	0.722084
0.451313	0.009067	0.050048	0.000014	0.722074
0.567365	-0.005651	0.055053	-0.000008	0.722085
0.627000	-0.020694	0.060058	-0.000019	0.722077
0.614765	-0.018410	0.065062	-0.000017	0.722077
0.676099	-0.027637	0.070067	-0.000028	0.722081
0.629079	-0.036522	0.075072	-0.000020	0.722047
0.582599	-0.177381	0.080077	-0.000011	0.721754
0.589974	-0.181766	0.085082	-0.000012	0.721748
0.601628	-0.185007	0.090086	-0.000015	0.721746
0.686195	-0.196584	0.095091	-0.000030	0.721753
0.470884	-0.161753	0.100096	0.000010	0.721746
0.454035	-0.154954	0.105101	0.000013	0.721753
0.206836	-0.221699	0.110106	0.000059	0.721536
0.167864	-0.262176	0.115110	0.000066	0.721443
0.543343	-0.326788	0.120115	-0.000004	0.721447
0.555349	-0.333108	0.125120	-0.000006	0.721439
0.641738	-0.345131	0.130125	-0.000022	0.721446
0.455571	-0.410988	0.135130	0.000012	0.721251
0.509415	-0.484601	0.140134	0.000002	0.721125
0.624435	-0.503708	0.145139	-0.000019	0.721128
0.360705	-0.461083	0.150144	0.000030	0.721120
0.610059	-0.550139	0.155149	-0.000017	0.721032
0.568165	-0.619377	0.160154	-0.000009	0.720881
0.616909	-0.628904	0.165158	-0.000018	0.720880
0.448029	-0.597337	0.170163	0.000013	0.720883
0.455869	-0.730062	0.175168	0.000012	0.720624
0.469867	-0.772379	0.180173	0.000009	0.720546
0.321090	-0.747722	0.185178	0.000037	0.720543
0.332460	-0.802648	0.190182	0.000035	0.720439
0.246772	-0.893114	0.195187	0.000051	0.720231
0.179800	-0.886710	0.200192	0.000063	0.720220
0.495007	-0.958868	0.205197	0.000004	0.720188
0.294190	-1.069202	0.210202	0.000042	0.719901
0.177970	-1.048875	0.215206	0.000063	0.719900
0.340283	-1.099621	0.220211	0.000033	0.719857
0.252164	-1.215149	0.225216	0.000050	0.719599
0.291712	-1.216227	0.230221	0.000042	0.719610
0.032914	-1.230769	0.235226	0.000090	0.719491
0.165978	-1.365871	0.240230	0.000066	0.719271
0.327270	-1.391563	0.245235	0.000035	0.719278
0.189062	-1.483266	0.250240	0.000061	0.719048
0.228200	-1.531081	0.255245	0.000054	0.718968
0.045700	-1.531980	0.260250	0.000088	0.718902
-0.070730	-1.641894	0.265254	0.000110	0.718644
-0.083566	-1.637170	0.270259	0.000112	0.718649
-0.089107	-1.742871	0.275264	0.000113	0.718439
0.078924	-1.813054	0.280269	0.000082	0.718359
0.114922	-1.881573	0.285274	0.000075	0.718237
0.043695	-1.978477	0.290278	0.000088	0.718020
-0.054161	-1.976945	0.295283	0.000106	0.717989
-0.192456	-2.096184	0.300288	0.000132	0.717705
-0.100343	-2.108143	0.305293	0.000115	0.717714
-0.397853	-2.208363	0.310298	0.000170	0.717411
-0.886689	-2.135832	0.315302	0.000261	0.717382
-1.317226	-2.151357	0.320307	0.000341	0.717200
-2.527963	-1.996557	0.325312	0.000567	0.717080
-1.883673	-2.106087	0.330317	0.000447	0.717090
-2.324357	-2.185631	0.335322	0.000529	0.716778
-3.455319	-1.993773	0.340326	0.000739	0.716759
-3.187941	-2.038812	0.345331	0.000689	0.716764
-3.513436	-2.126418	0.350336	0.000750	0.716476
-4.098207	-2.033974	0.355341	0.000859	0.716453
-4.180534	-2.020151	0.360346	0.000874	0.716451
-4.040782	-2.126727	0.365350	0.000848	0.716290
-5.186674	-1.999341	0.370355	0.001061	0.716138
-5.127721	-2.013206	0.375360	0.001050	0.716131
-4.929404	-2.045277	0.380365	0.001013	0.716138
-5.117692	-2.095468	0.385370	0.001048	0.715972
-5.914152	-1.998427	0.390374	0.001196	0.715883
-5.577611	-2.056501	0.395379	0.001134	0.715887
-5.722966	-2.035545	0.400384	0.001161	0.715877
-6.096987	-2.063288	0.405389	0.001230	0.715691
-7.208634	-1.937713	0.410394	0.001437	0.715547
-6.553476	-2.057392	0.415398	0.001315	0.715541
-6.542477	-2.054799	0.420403	0.001313	0.715550
-7.229024	-1.935856	0.425408	0.001441	0.715544
-7.159738	-2.062279	0.430413	0.001428	0.715318
-7.720626	-2.004597	0.435418	0.001532	0.715234
-7.678715	-2.013690	0.440422	0.001524	0.715231
-7.587490	-2.026218	0.445427	0.001507	0.715238
-7.949089	-1.969054	0.450432	0.001575	0.715224
-7.536580	-2.135327	0.455437	0.001498	0.715040
-8.711207	-1.994208	0.460442	0.001716	0.714905
-8.637039	-2.006453	0.465446	0.001703	0.714907
-8.318328	-2.060020	0.470451	0.001643	0.714914
-8.823912	-1.974998	0.475456	0.001737	0.714904
-8.464849	-2.039688	0.480461	0.001670	0.714902
-8.858825	-2.117403	0.485466	0.001744	0.714609
-9.445790	-2.014105	0.490470	0.001853	0.714606
-9.567472	-1.990082	0.495475	0.001875	0.714611
-9.202775	-2.059275	0.500480	0.001808	0.714603
-9.303677	-2.036753	0.505485	0.001826	0.714612
-9.723581	-2.009092	0.510490	0.001904	0.714519
-10.376421	-2.014394	0.515494	0.002026	0.714277
-9.697475	-2.133089	0.520499	0.001899	0.714282
-10.663228	-1.964268	0.525504	0.002079	0.714275
-10.529561	-1.983656	0.530509	0.002054	0.714284
-10.153209	-2.053550	0.535514	0.001984	0.714279
-10.326287	-2.029291	0.540518	0.002016	0.714266
-10.763854	-2.098587	0.545523	0.002098	0.713973
-11.280075	-2.010401	0.550528	0.002194	0.713966
-11.302565	-2.001263	0.555533	0.002198	0.713976
-11.022179	-2.051939	0.560538	0.002146	0.713975
-11.579319	-1.954694	0.565542	0.002249	0.713971
-11.275066	-2.005459	0.570547	0.002193	0.713978
-11.325231	-2.071035	0.575552	0.002202	0.713830
-12.355867	-1.972469	0.580557	0.002394	0.713661
-12.141044	-2.012446	0.585562	0.002354	0.713658
-12.333995	-1.978711	0.590566	0.002390	0.713657
-12.419259	-1.960943	0.595571	0.002405	0.713662
-12.063777	-2.029278	0.600576	0.002339	0.713652
-12.001170	-2.035422	0.605581	0.002327	0.713662
-12.494735	-2.024476	0.610586	0.002419	0.713509
-13.431241	-1.932120	0.615590	0.002594	0.713361
-12.384665	-2.114012	0.620595	0.002399	0.713370
-13.010102	-2.007654	0.625600	0.002515	0.713360
-13.388146	-1.937800	0.630605	0.002585	0.713365
-12.736891	-2.053535	0.635610	0.002464	0.713366
-12.820877	-2.041097	0.640614	0.002480	0.713361
-13.424554	-2.069261	0.645619	0.002592	0.713091
-14.447309	-1.921602	0.650624	0.002782	0.713022
-14.057221	-1.987198	0.655629	0.002710	0.713030
-13.784748	-2.036819	0.660634	0.002659	0.713028
-14.363798	-1.937074	0.665638	0.002767	0.713022
-13.985978	-1.999817	0.670643	0.002696	0.713031
-14.011718	-2.000305	0.675648	0.002701	0.713021
-14.324740	-2.006353	0.680653	0.002759	0.712898
-15.106583	-1.959515	0.685658	0.002905	0.712714
-14.879803	-2.002563	0.690662	0.002862	0.712709
-15.174094	-1.945515	0.695667	0.002917	0.712718
-15.110910	-1.962080	0.700672	0.002905	0.712708
-14.644636	-2.041215	0.705677	0.002819	0.712716
-15.142666	-1.953157	0.710682	0.002911	0.712714
-15.477969	-1.895858	0.715686	0.002973	0.712710
-14.938772	-2.114396	0.720691	0.002873	0.712466
-15.803039	-2.000854	0.725696	0.003034	0.712385
-16.175364	-1.929158	0.730701	0.003103	0.712396
-15.801721	-1.997787	0.735706	0.003034	0.712392
-15.838177	-1.995498	0.740710	0.003040	0.712384
-15.720682	-2.012647	0.745715	0.003018	0.712392
-16.060856	-1.955889	0.750720	0.003082	0.712384
-16.145659	-2.049355	0.755725	0.003097	0.712168
-16.807122	-1.968561	0.760730	0.003221	0.712094
-16.805747	-1.969917	0.765734	0.003220	0.712092
-16.477908	-2.025841	0.770739	0.003159	0.712097
-16.965798	-1.942602	0.775744	0.003250	0.712090
-17.020195	-1.931514	0.780749	0.003260	0.712093
-16.718217	-1.986119	0.785754	0.003204	0.712091
-16.910096	-2.046285	0.790758	0.003239	0.711903
-17.753281	-1.964061	0.795763	0.003396	0.711768
-17.566266	-2.003625	0.800768	0.003361	0.711755
-17.410877	-2.025964	0.805773	0.003332	0.711766
-17.765176	-1.962181	0.810778	0.003398	0.711768
-17.687441	-1.979139	0.815782	0.003384	0.711761
-17.448852	-2.018419	0.820787	0.003339	0.711768
-17.772002	-2.056439	0.825792	0.003400	0.711577
-18.630504	-1.962998	0.830797	0.003559	0.711459
-18.467439	-1.992774	0.835802	0.003529	0.711457
-18.578314	-1.973735	0.840806	0.003549	0.711456
-18.700929	-1.948026	0.845811	0.003572	0.711464
-18.856924	-1.926270	0.850816	0.003601	0.711452
-18.663119	-1.957728	0.855821	0.003565	0.711458
-18.343850	-2.063036	0.860826	0.003506	0.711362
-19.691469	-1.936627	0.865830	0.003756	0.711135
-19.177974	-2.024665	0.870835	0.003661	0.711142
-19.486489	-1.974748	0.875840	0.003718	0.711132
-19.575871	-1.955041	0.880845	0.003735	0.711140
-19.383721	-1.989804	0.885850	0.003699	0.711139
-19.448978	-1.979168	0.890854	0.003711	0.711137
-19.346125	-2.018670	0.895859	0.003692	0.711095
-20.202323	-1.980136	0.900864	0.003851	0.710867
-20.133694	-1.988001	0.905869	0.003838	0.710876
-20.203678	-1.975974	0.910874	0.003851	0.710875
-20.376707	-1.949807	0.915878	0.003883	0.710866
-20.030291	-2.005415	0.920883	0.003819	0.710878
-19.941435	-2.025291	0.925888	0.003802	0.710870
-20.298213	-2.039248	0.930893	0.003869	0.710716
-21.305354	-1.948621	0.935898	0.004056	0.710538
-21.032506	-1.999447	0.940902	0.004005	0.710534
-20.845932	-2.028138	0.945907	0.003971	0.710543
-21.374916	-1.939668	0.950912	0.004069	0.710532
-21.102170	-1.986724	0.955917	0.004018	0.710535
-20.742069	-2.049699	0.960922	0.003951	0.710538
-21.333883	-2.044820	0.965926	0.004061	0.710337
-22.252409	-1.937006	0.970931	0.004232	0.710225
-22.227658	-1.946314	0.975936	0.004227	0.710215
-22.184072	-1.950189	0.980941	0.004219	0.710223
-22.142237	-1.960198	0.985946	0.004211	0.710218
-22.079265	-1.972372	0.990950	0.004200	0.710217
-22.046123	-1.973567	0.995955	0.004193	0.710226
-22.249295	-1.964637	1.000960	0.004231	0.710172
-23.016649	-1.965859	1.005965	0.004374	0.709896
-22.723958	-2.016044	1.010970	0.004319	0.709900
-23.406497	-1.897739	1.015974	0.004446	0.709894
-22.919393	-1.981282	1.020979	0.004356	0.709900
-22.724904	-2.020096	1.025984	0.004319	0.709892
-23.154266	-1.942070	1.030989	0.004399	0.709895
-23.217322	-1.930613	1.035994	0.004411	0.709896
-23.494537	-2.001213	1.040998	0.004463	0.709656
-23.753156	-1.980933	1.046003	0.004511	0.709604
-23.848103	-1.969958	1.051008	0.004528	0.709592
-24.116845	-1.919308	1.056013	0.004578	0.709598
-23.846066	-1.965824	1.061018	0.004528	0.709602
-23.732359	-1.989810	1.066022	0.004507	0.709594
-23.713840	-1.987661	1.071027	0.004503	0.709605
-24.417731	-1.991804	1.076032	0.004634	0.709346
-24.978157	-1.932389	1.081037	0.004738	0.709265
-24.808176	-1.962853	1.086042	0.004707	0.709265
-24.817749	-1.963502	1.091046	0.004708	0.709261
-24.645047	-1.990044	1.096051	0.004676	0.709269
-24.932279	-1.943237	1.101056	0.004730	0.709260
-24.812324	-1.962406	1.106061	0.004707	0.709265
-24.763533	-2.038822	1.111066	0.004698	0.709130
-26.086920	-1.891253	1.116070	0.004944	0.708953
-25.432608	-2.004101	1.121075	0.004823	0.708961
-25.528939	-1.991665	1.126080	0.004840	0.708951
-25.687683	-1.959956	1.131085	0.004870	0.708958
-25.907249	-1.920371	1.136090	0.004911	0.708959
-26.082566	-1.892609	1.141094	0.004943	0.708952
-25.536975	-2.021634	1.146099	0.004842	0.708889
-26.511479	-1.974285	1.151104	0.005023	0.708636
-26.702044	-1.939946	1.156109	0.005059	0.708637
-26.651074	-1.948577	1.161114	0.005049	0.708638
-26.593585	-1.961254	1.166118	0.005038	0.708633
-26.778336	-1.922495	1.171123	0.005073	0.708645
-26.882855	-1.908947	1.176128	0.005092	0.708635
-26.568464	-1.963320	1.181133	0.005033	0.708638
-26.699092	-2.061457	1.186138	0.005058	0.708395
-27.769037	-1.895157	1.191142	0.005257	0.708346
-27.685177	-1.905756	1.196147	0.005241	0.708355
-27.688227	-1.908966	1.201152	0.005242	0.708348
-27.623191	-1.918624	1.206157	0.005229	0.708352
-27.212942	-1.991369	1.211162	0.005153	0.708352
-27.483074	-1.944835	1.216166	0.005203	0.708349
-27.952490	-1.981795	1.221171	0.005291	0.708108
-28.322695	-1.963054	1.226176	0.005360	0.708013
-28.189882	-1.987247	1.231181	0.005335	0.708012
-28.262767	-1.972596	1.236186	0.005348	0.708016
-28.803244	-1.878224	1.241190	0.005449	0.708012
-28.250491	-1.971972	1.246195	0.005346	0.708021
-28.132478	-1.997731	1.251200	0.005324	0.708012
-28.956302	-1.972823	1.256205	0.005477	0.707768
-29.566524	-1.895515	1.261210	0.005591	0.707705
-29.412416	-1.926967	1.266214	0.005562	0.707697
-29.014362	-1.993106	1.271219	0.005488	0.707707
-29.377547	-1.932784	1.276224	0.005555	0.707698
-29.437718	-1.920478	1.281229	0.005566	0.707701
-29.419134	-1.922988	1.286234	0.005563	0.707703
-29.438475	-1.974264	1.291238	0.005567	0.707593
-30.181970	-1.947763	1.296243	0.005705	0.707381
-29.982105	-1.988070	1.301248	0.005668	0.707371
-30.642791	-1.868104	1.306253	0.005791	0.707376
-30.051354	-1.970895	1.311258	0.005680	0.707381
-30.010326	-1.982229	1.316262	0.005673	0.707373
-30.563805	-1.880010	1.321267	0.005776	0.707381
-30.552833	-1.891549	1.326272	0.005774	0.707361
-30.592073	-2.024677	1.331277	0.005781	0.707080
-30.976464	-1.955319	1.336282	0.005852	0.707082
-31.565852	-1.852881	1.341286	0.005962	0.707077
-30.792745	-1.987669	1.346291	0.005818	0.707083
-31.035411	-1.947889	1.351296	0.005863	0.707076
-31.548073	-1.855084	1.356301	0.005959	0.707079
-31.140368	-1.925749	1.361306	0.005883	0.707083
-31.416156	-2.028159	1.366310	0.005934	0.706779
-31.862840	-1.960792	1.371315	0.006017	0.706755
-32.339137	-1.878626	1.376320	0.006106	0.706749
-32.000351	-1.938059	1.381325	0.006043	0.706751
-32.089907	-1.921760	1.386330	0.006059	0.706752
-32.248087	-1.897115	1.391334	0.006089	0.706745
-31.826040	-1.966570	1.396339	0.006010	0.706757
-32.404971	-1.979210	1.401344	0.006118	0.706524
-33.181879	-1.880745	1.406349	0.006262	0.706444
-32.668394	-1.970816	1.411354	0.006167	0.706447
-32.649269	-1.978163	1.416358	0.006163	0.706439
-33.235386	-1.869892	1.421363	0.006272	0.706447
-33.269735	-1.866852	1.426368	0.006278	0.706441
-32.856122	-1.939664	1.431373	0.006201	0.706443
-32.959021	-2.006311	1.436378	0.006220	0.706272
-34.307126	-1.841145	1.441382	0.006471	0.706121
-33.547021	-1.970910	1.446387	0.006330	0.706133
-33.537803	-1.976062	1.451392	0.006328	0.706126
-34.194539	-1.858968	1.456397	0.006450	0.706126
-33.799321	-1.928852	1.461402	0.006377	0.706127
-33.731492	-1.944879	1.466406	0.006364	0.706119
-33.889514	-1.965328	1.471411	0.006393	0.706022
-34.754890	-1.892274	1.476416	0.006554	0.705858
-34.449066	-1.945798	1.481421	0.006497	0.705861
-34.533110	-1.929511	1.486426	0.006513	0.705863
-34.821403	-1.879880	1.491430	0.006567	0.705860
-34.435040	-1.945897	1.496435	0.006495	0.705866
-34.236019	-1.984728	1.501440	0.006458	0.705859
-34.665971	-2.029778	1.506445	0.006538	0.705614
-35.574236	-1.912373	1.511450	0.006707	0.705525
-35.429188	-1.943249	1.516454	0.006679	0.705515
-35.206068	-1.977259	1.521459	0.006638	0.705527
-35.430686	-1.939520	1.526464	0.006680	0.705522
-35.146838	-1.988546	1.531469	0.006627	0.705525
-34.868800	-2.083351	1.536474	0.006575	0.705434
-36.775900	-1.857856	1.541478	0.006930	0.705204
-36.087477	-1.974356	1.546483	0.006802	0.705217
-36.160071	-1.965267	1.551488	0.006815	0.705209
-36.468702	-1.910378	1.556493	0.006873	0.705209
-36.249222	-1.947659	1.561498	0.006832	0.705213
-36.295022	-1.943812	1.566502	0.006840	0.705204
-36.198366	-2.011263	1.571507	0.006822	0.705103
-37.371740	-1.910812	1.576512	0.007040	0.704884
-37.183238	-1.944045	1.581517	0.007005	0.704885
-37.235690	-1.931569	1.586522	0.007015	0.704892
-37.392583	-1.907722	1.591526	0.007044	0.704883
-37.088668	-1.957422	1.596531	0.006988	0.704893
-37.039655	-1.970127	1.601536	0.006978	0.704885
-37.220839	-1.973646	1.606541	0.007012	0.704813
-37.963031	-1.950015	1.611546	0.007150	0.704594
-37.784793	-1.986493	1.616550	0.007117	0.704584
-37.916113	-1.958022	1.621555	0.007141	0.704595
-38.238015	-1.903553	1.626560	0.007201	0.704589
-37.936244	-1.957445	1.631565	0.007145	0.704589
-37.822807	-1.976289	1.636570	0.007124	0.704592
-38.383160	-1.960913	1.641574	0.007228	0.704422
-39.462258	-1.847108	1.646579	0.007429	0.704263
-38.694411	-1.986185	1.651584	0.007286	0.704259
-38.758209	-1.976220	1.656589	0.007298	0.704256
-39.163008	-1.899652	1.661594	0.007373	0.704265
-39.196721	-1.897683	1.666598	0.007379	0.704257
-38.813361	-1.963954	1.671603	0.007308	0.704261
-38.959558	-1.972708	1.676608	0.007335	0.704191
-39.909320	-1.922954	1.681613	0.007512	0.703950
-39.396185	-2.012790	1.686618	0.007416	0.703954
-39.922575	-1.921859	1.691622	0.007514	0.703948
-39.939905	-1.914218	1.696627	0.007517	0.703957
-39.727332	-1.954183	1.701632	0.007478	0.703953
-40.003576	-1.905411	1.706637	0.007529	0.703952
-39.924295	-1.944946	1.711642	0.007514	0.703901
-40.569367	-1.964313	1.716646	0.007634	0.703630
-40.451270	-1.979582	1.721651	0.007612	0.703642
-41.092639	-1.870352	1.726656	0.007732	0.703632
-40.905782	-1.903295	1.731661	0.007697	0.703633
-40.252208	-2.015543	1.736666	0.007575	0.703641
-40.813031	-1.922105	1.741670	0.007679	0.703628
-40.819916	-1.945762	1.746675	0.007681	0.703578
-41.364775	-1.967427	1.751680	0.007782	0.703338
-41.055084	-2.022310	1.756685	0.007724	0.703339
-41.484284	-1.943906	1.761690	0.007804	0.703343
-41.600882	-1.926998	1.766694	0.007826	0.703335
-41.145583	-2.003899	1.771699	0.007741	0.703344
-41.229919	-1.992202	1.776704	0.007757	0.703338
-41.906582	-1.999637	1.781709	0.007883	0.703079
-42.262419	-1.970911	1.786714	0.007949	0.703009
-42.368396	-1.957364	1.791718	0.007968	0.702998
-42.321073	-1.962377	1.796723	0.007960	0.703005
-42.551194	-1.924414	1.801728	0.008002	0.702999
-42.419818	-1.947853	1.806733	0.007978	0.702999
-42.333343	-1.959152	1.811738	0.007962	0.703008
-42.820785	-1.999293	1.816742	0.008052	0.702751
-43.006136	-1.994921	1.821747	0.008087	0.702693
-43.369491	-1.932969	1.826752	0.008154	0.702688
-43.422190	-1.923858	1.831757	0.008164	0.702687
-43.011745	-1.994507	1.836762	0.008088	0.702693
-43.004975	-2.001098	1.841766	0.008086	0.702682
-43.260283	-1.954432	1.846771	0.008134	0.702684
-43.869838	-2.003238	1.851776	0.008247	0.702366
-43.988497	-1.983369	1.856781	0.008269	0.702363
-44.125494	-1.955173	1.861786	0.008295	0.702371
-44.392576	-1.911928	1.866790	0.008345	0.702362
-44.131199	-1.953838	1.871795	0.008296	0.702372
-43.907804	-1.995153	1.876800	0.008254	0.702369
-44.281157	-1.930141	1.881805	0.008324	0.702366
-44.556742	-2.019433	1.886810	0.008375	0.702086
-44.903196	-1.969287	1.891814	0.008439	0.702063
-44.915720	-1.961319	1.896819	0.008442	0.702075
-44.732054	-1.995550	1.901824	0.008407	0.702072
-45.049838	-1.939712	1.906829	0.008466	0.702070
-44.902311	-1.961208	1.911834	0.008439	0.702080
-45.158925	-1.943868	1.916838	0.008487	0.702023
-45.573732	-2.008495	1.921843	0.008564	0.701742
-45.586776	-2.007032	1.926848	0.008566	0.701741
-46.031951	-1.929286	1.931853	0.008649	0.701738
-45.543709	-2.012350	1.936858	0.008558	0.701746
-45.563792	-2.013374	1.941862	0.008562	0.701737
-45.815331	-1.962982	1.946867	0.008609	0.701748
-45.922796	-2.012446	1.951872	0.008629	0.701609
-46.675285	-1.967041	1.956877	0.008769	0.701429
-46.225579	-2.043083	1.961882	0.008685	0.701438
-47.016830	-1.906398	1.966886	0.008832	0.701429
-46.849753	-1.932467	1.971891	0.008801	0.701437
-46.315786	-2.028315	1.976896	0.008701	0.701436
-46.844131	-1.934617	1.981901	0.008800	0.701435
-47.093083	-1.970228	1.986906	0.008846	0.701273
-47.866595	-1.910082	1.991910	0.008990	0.701115
-47.440398	-1.981666	1.996915	0.008911	0.701124
-47.659894	-1.944781	2.001920	0.008951	0.701120

-47.664955	-1.944139	2.011917	0.008952	0.701120
-47.540990	-1.965619	2.021914	0.008929	0.701121
-47.668970	-1.951470	2.031910	0.008953	0.701104
-47.972131	-2.010702	2.041907	0.009009	0.700875
-48.345343	-1.944680	2.051904	0.009078	0.700874
-48.046405	-1.998019	2.061901	0.009023	0.700874
-47.682416	-1.943404	2.071898	0.008955	0.701116
-47.639548	-1.947529	2.081894	0.008947	0.701123
-47.516296	-1.971582	2.091891	0.008924	0.701120
-47.531695	-1.968596	2.101888	0.008926	0.701120
-47.643576	-1.948250	2.111885	0.008947	0.701121
-47.450529	-1.982820	2.121882	0.008911	0.701121
-47.669116	-1.943679	2.131878	0.008952	0.701122
-47.576038	-1.961618	2.141875	0.008934	0.701119
-47.114671	-1.945977	2.151872	0.008848	0.701318
-46.526146	-1.992744	2.161869	0.008739	0.701436
-46.776627	-1.947993	2.171866	0.008785	0.701436
-46.705587	-1.960381	2.181862	0.008772	0.701437
-46.561406	-1.988785	2.191859	0.008745	0.701432
-45.986764	-1.945796	2.201856	0.008638	0.701726
-45.766928	-1.978306	2.211853	0.008597	0.701740
-45.901214	-1.951687	2.221850	0.008621	0.701746
-46.133601	-1.901550	2.231846	0.008665	0.701763
-45.069040	-1.940707	2.241843	0.008466	0.702068
-44.951314	-1.961458	2.251840	0.008444	0.702069
-44.765093	-1.992684	2.261837	0.008410	0.702073
-44.862947	-1.949839	2.271834	0.008428	0.702125
-43.966328	-1.988384	2.281830	0.008261	0.702371
-44.026112	-1.979416	2.291827	0.008272	0.702367
-44.183845	-1.950393	2.301824	0.008301	0.702369
-44.130964	-1.883109	2.311821	0.008291	0.702525
-43.245853	-1.957585	2.321818	0.008126	0.702693
-43.597321	-1.894676	2.331814	0.008191	0.702694
-43.331413	-1.913110	2.341811	0.008142	0.702753
-42.394268	-1.956554	2.351808	0.007967	0.703003
-42.275715	-1.975748	2.361805	0.007945	0.703007
-42.411946	-1.951875	2.371802	0.007970	0.703006
-41.858215	-1.957215	2.381798	0.007867	0.703195
-41.529146	-1.945041	2.391795	0.007806	0.703338
-41.494800	-1.950265	2.401792	0.007799	0.703340
-41.510986	-1.948144	2.411789	0.007802	0.703339
-40.612781	-1.970434	2.421786	0.007635	0.703617
-40.675988	-1.951371	2.431782	0.007646	0.703633
-40.354419	-2.008307	2.441779	0.007586	0.703634
-40.641908	-1.921021	2.451776	0.007640	0.703707
-39.397886	-2.023446	2.461773	0.007408	0.703948
-39.655434	-1.976589	2.471770	0.007456	0.703950
-39.591021	-1.987909	2.481766	0.007444	0.703951
-39.311899	-1.937989	2.491763	0.007392	0.704152
-38.711420	-1.993675	2.501760	0.007280	0.704256
-38.695783	-1.996376	2.511757	0.007277	0.704256
-38.808315	-1.963550	2.521754	0.007297	0.704282
-38.146634	-1.930437	2.531750	0.007174	0.704587
-37.804615	-1.991712	2.541747	0.007110	0.704587
-38.075811	-1.944363	2.551744	0.007161	0.704585
-37.487206	-1.949559	2.561741	0.007051	0.704786
-37.258654	-1.941098	2.571738	0.007008	0.704885
-37.044101	-1.978407	2.581734	0.006968	0.704888
-37.245268	-1.903925	2.591731	0.007006	0.704966
-36.250052	-1.960627	2.601728	0.006820	0.705209
-36.307373	-1.951020	2.611725	0.006831	0.705208
-36.458044	-1.923451	2.621722	0.006859	0.705209
-35.581903	-1.929091	2.631718	0.006695	0.705513
-35.336424	-1.967794	2.641715	0.006650	0.705523
-35.408318	-1.956716	2.651712	0.006663	0.705520
-35.080013	-1.929583	2.661709	0.006602	0.705692
-34.350358	-1.975178	2.671706	0.006466	0.705862
-34.485012	-1.952136	2.681702	0.006491	0.705861
-34.520147	-1.946252	2.691699	0.006497	0.705860
-33.742845	-1.967473	2.701696	0.006352	0.706096
-33.927438	-1.920020	2.711693	0.006386	0.706126
-33.726520	-1.956137	2.721690	0.006349	0.706125
-33.409784	-1.921224	2.731686	0.006290	0.706309
-32.993344	-1.930428	2.741683	0.006212	0.706440
-32.782234	-1.968595	2.751680	0.006173	0.706439
-32.754357	-1.942946	2.761677	0.006168	0.706501
-31.938727	-1.964228	2.771674	0.006016	0.706751
-32.074180	-1.940501	2.781670	0.006041	0.706750
-32.063168	-1.944711	2.791667	0.006038	0.706746
-31.552285	-1.903762	2.801664	0.005943	0.707011
-31.310205	-1.914672	2.811661	0.005898	0.707076
-31.048819	-1.962033	2.821658	0.005849	0.707075
-30.915594	-1.914135	2.831654	0.005824	0.707219
-30.496844	-1.912715	2.841651	0.005746	0.707372
-30.222914	-1.962272	2.851648	0.005695	0.707370
-30.448927	-1.902581	2.861645	0.005737	0.707409
-29.372032	-1.952762	2.871642	0.005536	0.707694
-29.470283	-1.935863	2.881638	0.005555	0.707693
-29.399190	-1.949382	2.891635	0.005541	0.707692
-29.069100	-1.905835	2.901632	0.005480	0.707897
-28.471345	-1.958227	2.911629	0.005368	0.708006
-28.524619	-1.947747	2.921626	0.005378	0.708008
-28.534088	-1.928390	2.931622	0.005380	0.708044
-27.825557	-1.905363	2.941619	0.005248	0.708343
-27.455355	-1.971374	2.951616	0.005179	0.708343
-27.886973	-1.892876	2.961613	0.005259	0.708347
-27.172927	-1.920391	2.971610	0.005126	0.708547
-27.023447	-1.901063	2.981606	0.005098	0.708639
-26.999035	-1.905911	2.991603	0.005093	0.708638
-26.921250	-1.855418	3.001600	0.005079	0.708767
-25.981875	-1.929975	3.011597	0.004904	0.708954
-26.084691	-1.911289	3.021594	0.004923	0.708954
-26.047368	-1.911724	3.031590	0.004916	0.708967
-25.148654	-1.924958	3.041587	0.004748	0.709261
-24.914179	-1.967479	3.051584	0.004704	0.709260
-25.076498	-1.937680	3.061581	0.004735	0.709262
-24.784945	-1.925264	3.071578	0.004680	0.709391
-24.159390	-1.934774	3.081574	0.004564	0.709595
-24.153686	-1.937147	3.091571	0.004562	0.709593
-24.445148	-1.885819	3.101568	0.004616	0.709592
-23.401063	-1.934629	3.111565	0.004422	0.709867
-23.189290	-1.958952	3.121562	0.004382	0.709894
-23.345763	-1.931681	3.131558	0.004411	0.709893
-23.362007	-1.881356	3.141555	0.004414	0.709988
-22.514076	-1.920194	3.151552	0.004256	0.710212
-22.482405	-1.923911	3.161549	0.004250	0.710216
-22.171918	-1.979116	3.171546	0.004192	0.710217
-21.870754	-1.908659	3.181542	0.004136	0.710465
-21.550579	-1.933388	3.191539	0.004077	0.710530
-21.558537	-1.932781	3.201536	0.004078	0.710528
-21.441313	-1.906627	3.211533	0.004056	0.710622
-20.461133	-1.956941	3.221530	0.003873	0.710871
-20.501670	-1.948963	3.231526	0.003881	0.710873
-20.452457	-1.959914	3.241523	0.003872	0.710869
-20.299329	-1.915741	3.251520	0.003843	0.711011
-19.632526	-1.972488	3.261517	0.003719	0.711136
-19.780211	-1.944358	3.271514	0.003746	0.711139
-20.013060	-1.879396	3.281510	0.003789	0.711186
-18.980037	-1.928751	3.291507	0.003597	0.711455
-19.184871	-1.893415	3.301504	0.003635	0.711453
-18.982285	-1.930092	3.311501	0.003597	0.711452
-18.565907	-1.872763	3.321498	0.003519	0.711715
-18.088139	-1.934720	3.331494	0.003430	0.711761
-18.127043	-1.927582	3.341491	0.003437	0.711762
-17.968274	-1.873026	3.351488	0.003408	0.711927
-17.174998	-1.933119	3.361485	0.003260	0.712089
-17.253851	-1.916940	3.371482	0.003274	0.712094
-17.233767	-1.915449	3.381478	0.003271	0.712104
-16.407614	-1.922413	3.391475	0.003117	0.712384
-16.416405	-1.919658	3.401472	0.003118	0.712386
-16.158630	-1.966324	3.411469	0.003070	0.712385
-16.239256	-1.874215	3.421466	0.003085	0.712540
-15.266631	-1.963555	3.431462	0.002904	0.712708
-15.546312	-1.914143	3.441459	0.002956	0.712707
-15.449743	-1.931888	3.451456	0.002938	0.712706
-14.465917	-1.949064	3.461453	0.002754	0.713021
-14.563664	-1.930970	3.471450	0.002772	0.713023
-14.500542	-1.942324	3.481446	0.002761	0.713023
-14.576459	-1.860173	3.491443	0.002775	0.713159
-13.577928	-1.937896	3.501440	0.002589	0.713359
-13.526949	-1.944807	3.511437	0.002579	0.713363
-13.701362	-1.914075	3.521434	0.002611	0.713363
-12.907866	-1.934797	3.531430	0.002463	0.713603
-13.139342	-1.870747	3.541427	0.002506	0.713649
-12.869199	-1.919299	3.551424	0.002456	0.713648
-12.718271	-1.869521	3.561421	0.002428	0.713801
-12.051888	-1.904128	3.571418	0.002304	0.713968
-12.061500	-1.902483	3.581414	0.002305	0.713968
-12.325132	-1.820502	3.591411	0.002354	0.714038
-10.972655	-1.942063	3.601408	0.002102	0.714275
-10.928340	-1.949357	3.611405	0.002094	0.714277
-10.767214	-1.976557	3.621402	0.002064	0.714280
-10.659009	-1.918464	3.631398	0.002044	0.714434
-9.663338	-2.008306	3.641395	0.001858	0.714608
-9.967889	-1.954864	3.651392	0.001915	0.714606
-9.771209	-1.989302	3.661389	0.001878	0.714608
-9.779171	-1.925556	3.671386	0.001879	0.714732
-8.722855	-2.022930	3.681382	0.001683	0.714912
-9.120095	-1.952898	3.691379	0.001756	0.714911
-8.772231	-2.016513	3.701376	0.001692	0.714908
-8.746036	-1.932906	3.711373	0.001687	0.715083
-7.733019	-2.036818	3.721370	0.001498	0.715235
-7.963385	-1.996713	3.731366	0.001541	0.715234
-7.832221	-2.020029	3.741363	0.001516	0.715234
-7.504639	-1.996257	3.751360	0.001455	0.715397
-6.931152	-2.023603	3.761357	0.001348	0.715546
-7.231518	-1.968941	3.771354	0.001404	0.715548
-7.095181	-1.993848	3.781350	0.001378	0.715547
-6.633287	-1.928233	3.791347	0.001292	0.715841
-5.996057	-2.020206	3.801344	0.001174	0.715884
-6.049550	-2.010389	3.811341	0.001183	0.715884
-5.983432	-2.002516	3.821338	0.001171	0.715923
-5.493165	-1.982903	3.831334	0.001080	0.716136
-5.013874	-2.067205	3.841331	0.000990	0.716138
-5.454447	-1.990409	3.851328	0.001072	0.716135
-4.862927	-2.017961	3.861325	0.000962	0.716289
-4.268533	-2.041940	3.871322	0.000851	0.716452
-4.353470	-2.028575	3.881318	0.000867	0.716448
-4.522039	-1.999168	3.891315	0.000898	0.716447
-3.472724	-2.042411	3.901312	0.000703	0.716732
-3.499281	-2.026258	3.911309	0.000707	0.716755
-3.291391	-2.063988	3.921306	0.000669	0.716753
-3.568979	-1.977411	3.931302	0.000720	0.716827
-2.578490	-2.024156	3.941299	0.000536	0.717084
-2.752809	-1.995385	3.951296	0.000568	0.717080
-2.621906	-2.018177	3.961293	0.000543	0.717081
-2.018644	-2.017198	3.971290	0.000431	0.717296
-1.772440	-2.016738	3.981286	0.000385	0.717383
-1.768646	-2.020010	3.991283	0.000384	0.717379
-1.701238	-1.987895	4.001280	0.000372	0.717466
-1.352443	-1.930694	4.011277	0.000306	0.717702
-1.107104	-1.973313	4.021274	0.000261	0.717704
-1.153344	-1.936357	4.031270	0.000269	0.717761
-1.102010	-1.816114	4.041267	0.000259	0.718017
-0.843634	-1.861093	4.051264	0.000211	0.718020
-0.854800	-1.772289	4.061261	0.000213	0.718191
-0.848616	-1.690195	4.071258	0.000212	0.718356
-0.792839	-1.658994	4.081254	0.000201	0.718437
-0.916425	-1.532023	4.091251	0.000224	0.718645
-0.837476	-1.497289	4.101248	0.000209	0.718741
-0.825301	-1.388710	4.111245	0.000207	0.718960
-0.719115	-1.319226	4.121242	0.000187	0.719134
-0.698608	-1.252730	4.131238	0.000183	0.719273
-0.689632	-1.100962	4.141235	0.000181	0.719576
-0.592807	-1.048331	4.151232	0.000163	0.719714
-0.640501	-0.945638	4.161229	0.000172	0.719899
-0.461978	-0.819167	4.171226	0.000138	0.720211
-0.390770	-0.732661	4.181222	0.000125	0.720407
-0.253992	-0.646886	4.191219	0.000099	0.720624
-0.294356	-0.511262	4.201216	0.000106	0.720877
-0.399972	-0.372476	4.211213	0.000126	0.721113
-0.132025	-0.290554	4.221210	0.000076	0.721368
-0.191639	-0.149422	4.231206	0.000087	0.721625
0.043763	-0.053656	4.241203	0.000043	0.721896
-0.025768	0.103503	4.251200	0.000055	0.722180
0.000000	0.281137	4.261197	0.000050	0.722538

-0.038250	0.926966	4.266202	0.000057	0.723792
0.198168	2.145192	4.271206	0.000012	0.726258
0.351287	3.973067	4.276211	-0.000018	0.729872
0.680910	6.322011	4.281216	-0.000081	0.734536
0.895414	9.203453	4.286221	-0.000122	0.740152
1.050727	12.570432	4.291226	-0.000154	0.746629
1.646532	16.320021	4.296230	-0.000267	0.753918
1.993100	20.513009	4.301235	-0.000334	0.761880
2.238170	25.125635	4.306240	-0.000383	0.770500
2.566020	30.096885	4.311245	-0.000447	0.779703
3.154126	35.357453	4.316250	-0.000560	0.789402
3.649824	40.967299	4.321254	-0.000656	0.799573
4.005769	46.897241	4.326259	-0.000727	0.810134
4.601028	53.070749	4.331264	-0.000841	0.821052
5.122082	59.534039	4.336269	-0.000943	0.832299
5.632310	66.211353	4.341274	-0.001042	0.843752
6.632495	73.044183	4.346278	-0.001233	0.855452
7.513302	80.097580	4.351283	-0.001402	0.867320
8.241818	87.379275	4.356288	-0.001542	0.879352
9.240281	94.790322	4.361293	-0.001733	0.891503
9.782690	102.438995	4.366298	-0.001839	0.903737
10.768068	110.173376	4.371302	-0.002027	0.916061
11.576989	118.040223	4.376307	-0.002183	0.928375
11.987155	126.107927	4.381312	-0.002265	0.940725
12.893987	134.195200	4.386317	-0.002439	0.953073
13.075825	142.477304	4.391322	-0.002478	0.965363
14.023371	150.730613	4.396326	-0.002660	0.977650
14.868562	159.079797	4.401331	-0.002823	0.989896
15.322439	167.538089	4.406336	-0.002913	1.002050
16.214066	175.968537	4.411341	-0.003085	1.014125
16.809928	184.472930	4.416346	-0.003201	1.026089
17.639816	192.990257	4.421350	-0.003361	1.037988
18.332632	201.541320	4.426355	-0.003496	1.049765
19.044108	210.131244	4.431360	-0.003634	1.061467
19.699391	218.760839	4.436365	-0.003762	1.073081
20.136615	227.411336	4.441370	-0.003849	1.084548
20.647791	236.075607	4.446374	-0.003950	1.095929
21.279261	244.699279	4.451379	-0.004073	1.107167
22.079325	253.324421	4.456384	-0.004228	1.118331
22.741315	261.962408	4.461389	-0.004357	1.129370
23.233944	270.617807	4.466394	-0.004454	1.140288
24.245862	279.219276	4.471398	-0.004648	1.151144
24.835681	287.856572	4.476403	-0.004764	1.161855
25.299977	296.506113	4.481408	-0.004856	1.172456
25.812289	305.125600	4.486413	-0.004957	1.182936
26.674041	313.682165	4.491418	-0.005123	1.193319
27.312514	322.273766	4.496422	-0.005248	1.203609
27.730761	330.885475	4.501427	-0.005331	1.213791
28.369873	339.445879	4.506432	-0.005456	1.223873
28.839344	348.052469	4.511437	-0.005549	1.233891
29.220724	356.606164	4.516442	-0.005626	1.243752
29.902345	365.116198	4.521446	-0.005758	1.253542
30.552240	373.607692	4.526451	-0.005885	1.263230
30.991287	382.135650	4.531456	-0.005972	1.272845
31.693182	390.600267	4.536461	-0.006108	1.282366
32.269382	399.073542	4.541466	-0.006221	1.291803
32.943092	407.534897	4.546470	-0.006352	1.301176
33.419278	416.069615	4.551475	-0.006446	1.310525
34.068282	424.561209	4.556480	-0.006573	1.319793
34.393966	433.012306	4.561485	-0.006639	1.328895
34.763036	441.443565	4.566490	-0.006713	1.337921
35.412289	449.814378	4.571494	-0.006840	1.346873
35.862744	458.225006	4.576499	-0.006929	1.355772
36.419457	466.576294	4.581504	-0.007038	1.364569
37.308192	474.908711	4.586509	-0.007209	1.373348
37.777657	483.278203	4.591514	-0.007302	1.382036
37.845058	491.741746	4.596518	-0.007320	1.390699
38.215746	500.109167	4.601523	-0.007395	1.399261
38.825113	508.419780	4.606528	-0.007514	1.407753
39.350048	516.761508	4.611533	-0.007617	1.416212
39.603829	525.108675	4.616538	-0.007670	1.424580
40.260356	533.433231	4.621542	-0.007798	1.432944
40.854040	541.719660	4.626547	-0.007914	1.441210
41.253296	550.045224	4.631552	-0.007993	1.449437
41.929929	558.339549	4.636557	-0.008125	1.457630
42.304315	566.633643	4.641562	-0.008200	1.465730
42.751110	574.995449	4.646566	-0.008289	1.473861
42.876846	583.316299	4.651571	-0.008318	1.481858
43.267794	591.581174	4.656576	-0.008396	1.489800
43.970287	599.826125	4.661581	-0.008532	1.497729
44.447980	608.062197	4.666586	-0.008626	1.505573
45.022377	616.333142	4.671590	-0.008739	1.513424
45.393217	624.586780	4.676595	-0.008813	1.521187
45.763154	632.856477	4.681600	-0.008888	1.528925
46.536673	641.070710	4.686605	-0.009037	1.536634
46.917063	649.326151	4.691610	-0.009113	1.544283
47.134630	657.636952	4.696614	-0.009159	1.551920
47.394807	665.898789	4.701619	-0.009213	1.559482
47.751823	674.114315	4.706624	-0.009285	1.566980
48.290282	682.352704	4.711629	-0.009391	1.574488
48.759258	690.544701	4.716634	-0.009483	1.581909
49.320751	698.758952	4.721638	-0.009593	1.589329
49.750720	706.990342	4.726643	-0.009679	1.596710
50.084417	715.202307	4.731648	-0.009746	1.604026
50.616101	723.412275	4.736653	-0.009851	1.611335
50.985903	731.635282	4.741658	-0.009925	1.618600
51.359418	739.849064	4.746662	-0.010000	1.625824
51.677999	748.123391	4.751667	-0.010065	1.633062
52.063131	756.318105	4.756672	-0.010142	1.640207
52.617200	764.478891	4.761677	-0.010251	1.647316
52.571657	772.738422	4.766682	-0.010247	1.654396
52.947772	780.923256	4.771686	-0.010323	1.661440
53.172667	789.115445	4.776691	-0.010370	1.668440
53.584284	797.300336	4.781696	-0.010452	1.675429
54.127066	805.448678	4.786701	-0.010559	1.682376
54.427603	813.627575	4.791706	-0.010620	1.689288
54.909676	821.810894	4.796710	-0.010715	1.696199
55.474072	829.948698	4.801715	-0.010826	1.703055
55.859289	838.136107	4.806720	-0.010903	1.709900
56.266664	846.335117	4.811725	-0.010984	1.716731
56.636939	854.471449	4.816730	-0.011058	1.723479
56.981204	862.644169	4.821734	-0.011128	1.730226
57.355740	870.818780	4.826739	-0.011203	1.736952
57.710166	878.984829	4.831744	-0.011274	1.743643
58.065482	887.156647	4.836749	-0.011346	1.750313
58.343896	895.332541	4.841754	-0.011403	1.756951
58.937770	903.459534	4.846758	-0.011519	1.763564
59.007791	911.661056	4.851763	-0.011537	1.770147
59.167022	919.851714	4.856768	-0.011572	1.776707
59.581605	927.991080	4.861773	-0.011655	1.783234
60.072377	936.126188	4.866778	-0.011752	1.789744
60.632618	944.306985	4.871782	-0.011861	1.796273
60.981054	952.421759	4.876787	-0.011932	1.802702
61.216657	960.569357	4.881792	-0.011981	1.809120
61.513063	968.736350	4.886797	-0.012041	1.815537
61.884890	976.850425	4.891802	-0.012116	1.821899
62.480329	984.952544	4.896806	-0.012232	1.828257
62.792486	993.121988	4.901811	-0.012296	1.834611
63.016069	1001.262252	4.906816	-0.012343	1.840910
63.638159	1009.369676	4.911821	-0.012464	1.847208
63.820873	1017.541872	4.916826	-0.012503	1.853484
64.082917	1025.698656	4.921830	-0.012557	1.859736
64.292621	1033.835617	4.926835	-0.012602	1.865945
64.465614	1042.023258	4.931840	-0.012639	1.872168
64.781521	1050.153997	4.936845	-0.012704	1.878344
65.013142	1058.252762	4.941850	-0.012752	1.884466
65.236713	1066.402247	4.946854	-0.012799	1.890604
65.536401	1074.529875	4.951859	-0.012860	1.896716
65.701934	1082.659468	4.956864	-0.012896	1.902794
66.243970	1090.760922	4.961869	-0.013003	1.908874
66.340334	1098.908851	4.966874	-0.013026	1.914919
66.573107	1107.024751	4.971878	-0.013075	1.920936
66.788097	1115.138846	4.976883	-0.013120	1.926931
67.133435	1123.255580	4.981888	-0.013190	1.932924
67.579638	1131.362552	4.986893	-0.013278	1.938903
67.994285	1139.422504	4.991898	-0.013361	1.944825
68.265704	1147.597300	4.996902	-0.013417	1.950797
68.255394	1155.780961	5.001907	-0.013420	1.956726
68.513210	1163.854536	5.006912	-0.013473	1.962587
68.975633	1171.934476	5.011917	-0.013565	1.968457
69.054343	1180.085149	5.016922	-0.013585	1.974319
69.690935	1188.121040	5.021926	-0.013709	1.980141
69.822773	1196.232886	5.026931	-0.013739	1.985946
70.174017	1204.357485	5.031936	-0.013809	1.991767
70.455355	1212.477345	5.036941	-0.013867	1.997560
70.671503	1220.560016	5.041946	-0.013913	2.003303
71.280417	1228.631590	5.046950	-0.014031	2.009062
71.636441	1236.741606	5.051955	-0.014103	2.014806
71.798016	1244.862148	5.056960	-0.014138	2.020521
72.080972	1252.974290	5.061965	-0.014196	2.026226
72.320556	1261.107199	5.066970	-0.014246	2.031925
72.680806	1269.211245	5.071974	-0.014319	2.037600
72.994020	1277.280445	5.076979	-0.014382	2.043230
73.212437	1285.383151	5.081984	-0.014428	2.048859
73.422233	1293.523641	5.086989	-0.014473	2.054497
73.833049	1301.574108	5.091994	-0.014555	2.060077
74.227833	1309.660028	5.096998	-0.014633	2.065666
74.515978	1317.771639	5.102003	-0.014692	2.071246
74.938925	1325.863044	5.107008	-0.014777	2.076811
75.242614	1333.947940	5.112013	-0.014838	2.082344
75.486529	1342.041185	5.117018	-0.014889	2.087862
75.724642	1350.174900	5.122022	-0.014939	2.093393
75.954029	1358.283450	5.127027	-0.014987	2.098891
76.371746	1366.332808	5.132032	-0.015070	2.104354
76.541469	1374.479770	5.137037	-0.015107	2.109843
76.798237	1382.624330	5.142042	-0.015160	2.115325
77.325460	1390.650188	5.147046	-0.015264	2.120739
77.491303	1398.728627	5.152051	-0.015300	2.126140
77.653606	1406.832256	5.157056	-0.015335	2.131544
78.160081	1414.910450	5.162061	-0.015435	2.136950
78.468918	1422.969096	5.167066	-0.015498	2.142310
78.593984	1431.090133	5.172070	-0.015526	2.147681
78.791199	1439.198728	5.177075	-0.015568	2.153036
79.276989	1447.243368	5.182080	-0.015664	2.158364
79.342011	1455.358268	5.187085	-0.015682	2.163685
79.640631	1463.413280	5.192090	-0.015743	2.168975
80.067347	1471.503785	5.197094	-0.015827	2.174288
80.307464	1479.583708	5.202099	-0.015877	2.179563
80.560118	1487.655595	5.207104	-0.015930	2.184822
81.038701	1495.738310	5.212109	-0.016024	2.190095
80.973923	1503.888936	5.217114	-0.016017	2.195350
81.444608	1511.926610	5.222118	-0.016110	2.200569
81.590514	1520.008865	5.227123	-0.016143	2.205774
81.915523	1528.080220	5.232128	-0.016209	2.210976
82.153362	1536.180165	5.237133	-0.016258	2.216176
82.268097	1544.248016	5.242138	-0.016285	2.221333
82.672975	1552.316594	5.247142	-0.016366	2.226503
83.121643	1560.398346	5.252147	-0.016455	2.231674
83.155306	1568.507653	5.257152	-0.016466	2.236814
83.417867	1576.567316	5.262157	-0.016520	2.241931
83.540611	1584.631391	5.267162	-0.016549	2.247026
84.054810	1592.695848	5.272166	-0.016650	2.252144
84.534806	1600.758642	5.277171	-0.016744	2.257247
84.745563	1608.834019	5.282176	-0.016789	2.262322
85.033914	1616.931683	5.287181	-0.016848	2.267407
85.278464	1625.064088	5.292186	-0.016899	2.272498
85.536531	1633.155764	5.297190	-0.016952	2.277554
85.932793	1641.175013	5.302195	-0.017031	2.282565
86.032092	1649.242037	5.307200	-0.017055	2.287569
86.506607	1657.300913	5.312205	-0.017149	2.292589
86.609996	1665.380187	5.317210	-0.017173	2.297579
86.896816	1673.438196	5.322214	-0.017232	2.302561
87.044401	1681.523549	5.327219	-0.017265	2.307537
87.029539	1689.634179	5.332224	-0.017267	2.312504
87.471820	1697.682848	5.337229	-0.017355	2.317461
87.622500	1705.737141	5.342234	-0.017388	2.322386
87.914578	1713.793470	5.347238	-0.017448	2.327314
88.061828	1721.884495	5.352243	-0.017481	2.332241
88.316954	1729.952028	5.357248	-0.017534	2.337151
88.573066	1738.025986	5.362253	-0.017587	2.342055
88.926994	1746.064691	5.367258	-0.017658	2.346936
89.409636	1754.151989	5.372262	-0.017753	2.351846
89.667926	1762.226803	5.377267	-0.017806	2.356720
89.871037	1770.280376	5.382272	-0.017850	2.361567
90.156698	1778.345777	5.387277	-0.017908	2.366417
90.166005	1786.422492	5.392282	-0.017915	2.371242
90.295833	1794.513630	5.397286	-0.017945	2.376076
90.679127	1802.545813	5.402291	-0.018021	2.380885
90.709815	1810.625448	5.407296	-0.018032	2.385684
90.959324	1818.720314	5.412301	-0.018084	2.390500
91.308337	1826.763678	5.417306	-0.018154	2.395283
91.763707	1834.785072	5.422310	-0.018244	2.400053
92.150322	1842.817301	5.427315	-0.018322	2.404813
92.600850	1850.861727	5.432320	-0.018411	2.409577
92.799899	1858.988823	5.437325	-0.018453	2.414359
92.961661	1867.045040	5.442330	-0.018489	2.419088
93.273827	1875.091864	5.447334	-0.018552	2.423814
93.691412	1883.141464	5.452339	-0.018635	2.428540
93.922545	1891.293675	5.457344	-0.018684	2.433303
94.337903	1899.334154	5.462349	-0.018766	2.438005
94.239069	1907.396163	5.467354	-0.018753	2.442671
94.577066	1915.428242	5.472358	-0.018821	2.447345
94.704745	1923.515964	5.477363	-0.018851	2.452025
94.862785	1931.563206	5.482368	-0.018885	2.456676
95.196678	1939.618809	5.487373	-0.018953	2.461335
95.592929	1947.622433	5.492378	-0.019032	2.465961
95.774275	1955.725010	5.497382	-0.019071	2.470619
96.096636	1963.795128	5.502387	-0.019136	2.475259
96.234697	1971.832076	5.507392	-0.019167	2.479859
96.409556	1979.894339	5.512397	-0.019205	2.484467
96.711283	1987.924193	5.517402	-0.019267	2.489057
97.148198	1995.999437	5.522406	-0.019353	2.493674
97.342122	2004.073398	5.527411	-0.019395	2.498265
97.682136	2012.090445	5.532416	-0.019463	2.502825
97.943987	2020.175304	5.537421	-0.019517	2.507409
98.003093	2028.273798	5.542426	-0.019534	2.511978
98.203678	2036.340014	5.547430	-0.019576	2.516531
98.599833	2044.369159	5.552435	-0.019655	2.521069
98.678989	2052.411017	5.557440	-0.019675	2.525583
98.898951	2060.481967	5.562445	-0.019722	2.530115
99.088598	2068.538964	5.567450	-0.019762	2.534629
99.242607	2076.586977	5.572454	-0.019796	2.539128
99.419906	2084.644717	5.577459	-0.019835	2.543625
99.729107	2092.670533	5.582464	-0.019898	2.548107
100.158694	2100.747218	5.587469	-0.019983	2.552616
100.342989	2108.799020	5.592474	-0.020022	2.557087
100.497492	2116.838843	5.597478	-0.020056	2.561542
100.947754	2124.865568	5.602483	-0.020146	2.566002
101.007965	2132.953509	5.607488	-0.020162	2.570460
101.296938	2141.040063	5.612493	-0.020221	2.574926
101.542206	2149.057244	5.617498	-0.020272	2.579343
101.921121	2157.094060	5.622502	-0.020348	2.583773
102.021495	2165.174136	5.627507	-0.020372	2.588199
102.185165	2173.355184	5.632512	-0.020408	2.592678
102.543209	2181.434458	5.637517	-0.020480	2.597106
102.683472	2189.442676	5.642522	-0.020511	2.601473
102.853772	2197.450922	5.647526	-0.020548	2.605835
102.990924	2205.479992	5.652531	-0.020579	2.610199
103.353890	2213.498276	5.657536	-0.020652	2.614564
103.492781	2221.571288	5.662541	-0.020683	2.618937
103.653060	2229.592697	5.667546	-0.020718	2.623276
104.009771	2237.603774	5.672550	-0.020790	2.627616
104.181177	2245.683154	5.677555	-0.020827	2.631972
104.330448	2253.739771	5.682560	-0.020860	2.636308
104.867326	2261.742796	5.687565	-0.020966	2.640633
105.058288	2269.779599	5.692570	-0.021006	2.644947
105.205194	2277.847332	5.697574	-0.021039	2.649267
105.329153	2285.931433	5.702579	-0.021068	2.653587
105.817227	2293.929686	5.707584	-0.021164	2.657878
106.166441	2301.986915	5.712589	-0.021234	2.662185
106.283389	2310.049231	5.717594	-0.021261	2.666472
106.576174	2318.105552	5.722598	-0.021321	2.670760
106.763873	2326.189546	5.727603	-0.021361	2.675050
106.933626	2334.211920	5.732608	-0.021398	2.679298
107.459577	2342.225308	5.737613	-0.021501	2.683558
107.735820	2350.249313	5.742618	-0.021558	2.687801
107.881302	2358.336427	5.747622	-0.021590	2.692062
108.029633	2366.408722	5.752627	-0.021623	2.696309
108.316223	2374.431289	5.757632	-0.021682	2.700531
108.649108	2382.468188	5.762637	-0.021749	2.704757
108.483749	2390.553118	5.767642	-0.021724	2.708971
108.849572	2398.597103	5.772646	-0.021797	2.713189
109.143718	2406.635404	5.777651	-0.021857	2.717394
109.221606	2414.676702	5.782656	-0.021877	2.721581
109.519614	2422.721045	5.787661	-0.021938	2.725776
109.845308	2430.746339	5.792666	-0.022004	2.729956
110.090163	2438.814257	5.797670	-0.022055	2.734147
110.214580	2446.875737	5.802675	-0.022083	2.738321
110.317494	2454.901887	5.807680	-0.022108	2.742469
110.483177	2462.969825	5.812685	-0.022144	2.746636
110.772029	2471.016146	5.817690	-0.022203	2.750792
111.039611	2479.139968	5.822694	-0.022258	2.754982
111.030289	2487.170607	5.827699	-0.022262	2.759100
111.202682	2495.158961	5.832704	-0.022299	2.763201
111.566957	2503.175895	5.837709	-0.022372	2.767323
111.801058	2511.236140	5.842714	-0.022421	2.771452
112.144712	2519.268781	5.847718	-0.022490	2.775568
112.269562	2527.318821	5.852723	-0.022519	2.779673
112.743822	2535.315559	5.857728	-0.022612	2.783766
113.139933	2543.372207	5.862733	-0.022691	2.787879
113.078066	2551.456540	5.867738	-0.022685	2.791972
113.417814	2559.508640	5.872742	-0.022754	2.796067
113.701564	2567.522957	5.877747	-0.022812	2.800134
113.796087	2575.551132	5.882752	-0.022835	2.804190
113.864208	2583.607678	5.887757	-0.022853	2.808253
114.224644	2591.636082	5.892762	-0.022925	2.812313
114.455001	2599.710522	5.897766	-0.022973	2.816383
114.633707	2607.747899	5.902771	-0.023012	2.820426
115.078971	2615.743311	5.907776	-0.023100	2.824456
115.276550	2623.818689	5.912781	-0.023142	2.828507
115.338120	2631.894388	5.917786	-0.023159	2.832545
115.690303	2639.926618	5.922790	-0.023230	2.836571
115.859107	2647.959958	5.927795	-0.023267	2.840582
116.017018	2655.946945	5.932800	-0.023301	2.844563
116.056596	2664.025934	5.937805	-0.023314	2.848578
116.483310	2672.044199	5.942810	-0.023399	2.852579
116.572909	2680.101951	5.947814	-0.023421	2.856575
116.704383	2688.156845	5.952819	-0.023451	2.860566
116.862496	2696.142265	5.957824	-0.023485	2.864519
117.279851	2704.199623	5.962829	-0.023568	2.868516
117.426145	2712.256999	5.967834	-0.023601	2.872493
117.531006	2720.314388	5.972838	-0.023626	2.876461
117.789869	2728.343490	5.977843	-0.023679	2.880419
117.874245	2736.351663	5.982848	-0.023700	2.884351
118.130805	2744.417332	5.987853	-0.023753	2.888316
118.450816	2752.457156	5.992858	-0.023818	2.892266
118.700500	2760.507644	5.997862	-0.023870	2.896212
118.889836	2768.554166	6.002867	-0.023910	2.900147
119.073730	2776.553968	6.007872	-0.023950	2.904054
119.327105	2784.627619	6.012877	-0.024002	2.907995
119.490002	2792.686972	6.017882	-0.024038	2.911919
119.856180	2800.781289	6.022886	-0.024112	2.915866
120.159196	2808.758947	6.027891	-0.024173	2.919747
120.281705	2816.774285	6.032896	-0.024201	2.923632
120.475778	2824.807394	6.037901	-0.024243	2.927524
120.794240	2832.837066	6.042906	-0.024307	2.931415
121.133854	2840.882412	6.047910	-0.024376	2.935310
121.472098	2848.911518	6.052915	-0.024444	2.939192
121.591544	2856.918656	6.057920	-0.024472	2.943047
121.945533	2864.981211	6.062925	-0.024543	2.946935
121.787677	2873.061157	6.067930	-0.024519	2.950800
121.975156	2881.092107	6.072934	-0.024559	2.954655
122.284010	2889.100953	6.077939	-0.024622	2.958500
122.469041	2897.119985	6.082944	-0.024662	2.962338
122.969161	2905.142510	6.087949	-0.024760	2.966190
123.107943	2913.179087	6.092954	-0.024791	2.970024
123.443489	2921.253003	6.097958	-0.024859	2.973881
123.573836	2929.315461	6.102963	-0.024888	2.977718
123.641972	2937.326545	6.107968	-0.024906	2.981522
123.838206	2945.348763	6.112973	-0.024948	2.985332
124.020053	2953.386833	6.117978	-0.024987	2.989145
124.305447	2961.455348	6.122982	-0.025046	2.992972
124.715962	2969.494617	6.127987	-0.025128	2.996787
124.606381	2977.509879	6.132992	-0.025112	3.000560
124.926029	2985.533669	6.137997	-0.025177	3.004353
125.138420	2993.565122	6.143002	-0.025222	3.008139
125.330298	3001.618950	6.148006	-0.025263	3.011931
125.526558	3009.689901	6.153011	-0.025305	3.015726
125.660378	3017.680961	6.158016	-0.025335	3.019475
125.800844	3025.734091	6.163021	-0.025367	3.023249
126.080199	3033.754116	6.168026	-0.025424	3.027010
126.193573	3041.819636	6.173030	-0.025450	3.030779
126.723882	3049.854586	6.178035	-0.025554	3.034550
126.981306	3057.852971	6.183040	-0.025608	3.038285
127.039604	3065.905488	6.188045	-0.025624	3.042032
127.143854	3073.931596	6.193050	-0.025648	3.045763
127.473974	3081.938907	6.198054	-0.025715	3.049493
127.737073	3090.015035	6.203059	-0.025769	3.053246
127.821431	3098.043315	6.208064	-0.025790	3.056964
128.215095	3106.069284	6.213069	-0.025869	3.060691
128.232979	3114.103800	6.218074	-0.025878	3.064400
128.383040	3122.144039	6.223078	-0.025911	3.068113
128.716569	3130.236454	6.228083	-0.025978	3.071854
128.830156	3138.315794	6.233088	-0.026005	3.075574
128.999101	3146.301401	6.238093	-0.026042	3.079249
129.260277	3154.298181	6.243098	-0.026095	3.082929
129.490222	3162.318047	6.248102	-0.026144	3.086614
129.680618	3170.357764	6.253107	-0.026184	3.090302
129.877630	3178.381914	6.258112	-0.026226	3.093978
130.362746	3186.405871	6.263117	-0.026322	3.097664
130.694769	3194.426931	6.268122	-0.026389	3.101336
130.653398	3202.460140	6.273126	-0.026387	3.104992
130.739017	3210.536106	6.278131	-0.026408	3.108670
130.735431	3218.589343	6.283136	-0.026412	3.112329
131.205831	3226.607555	6.288141	-0.026505	3.115988
131.217035	3234.615663	6.293146	-0.026513	3.119619
131.667143	3242.608149	6.298150	-0.026602	3.123257
131.843079	3250.673291	6.303155	-0.026640	3.126912
131.884477	3258.692804	6.308160	-0.026653	3.130536
132.021493	3266.795981	6.313165	-0.026684	3.134198
132.435433	3274.758721	6.318170	-0.026766	3.137805
132.723091	3282.786980	6.323174	-0.026825	3.141431
132.909036	3290.825618	6.328179	-0.026865	3.145053
133.059598	3298.861090	6.333184	-0.026898	3.148668
133.269515	3306.963454	6.338189	-0.026943	3.152311
133.504487	3314.976639	6.343194	-0.026992	3.155912
133.816002	3322.955347	6.348198	-0.027055	3.159496
134.150655	3330.958501	6.353203	-0.027122	3.163088
134.239188	3338.998992	6.358208	-0.027144	3.166681
134.542868	3347.045357	6.363213	-0.027206	3.170283
134.797241	3355.088263	6.368218	-0.027259	3.173877
135.051132	3363.096938	6.373222	-0.027311	3.177451
135.319635	3371.178724	6.378227	-0.027367	3.181054
135.393122	3379.142884	6.383232	-0.027385	3.184593
135.459052	3387.249101	6.388237	-0.027403	3.188191
135.516809	3395.310289	6.393242	-0.027419	3.191764
135.834193	3403.303528	6.398246	-0.027484	3.195314
136.361852	3411.328204	6.403251	-0.027587	3.198883
136.511760	3419.322296	6.408256	-0.027620	3.202418
136.605963	3427.393633	6.413261	-0.027643	3.205981
136.692507	3435.418702	6.418266	-0.027665	3.209520
136.957837	3443.448571	6.423270	-0.027719	3.213064
137.232291	3451.529230	6.428275	-0.027776	3.216627
137.067635	3459.530792	6.433280	-0.027750	3.220133
137.374140	3467.555899	6.438285	-0.027813	3.223664
137.391049	3475.577157	6.443290	-0.027821	3.227179
137.660414	3483.607134	6.448294	-0.027876	3.230704
138.083718	3491.705272	6.453299	-0.027961	3.234261
138.125128	3499.683535	6.458304	-0.027974	3.237746
138.407779	3507.690270	6.463309	-0.028031	3.241249
138.739184	3515.663294	6.468314	-0.028098	3.244736
139.119387	3523.706584	6.473318	-0.028175	3.248252
139.095382	3531.803997	6.478323	-0.028175	3.251771
139.231857	3539.807636	6.483328	-0.028206	3.255252
139.301236	3547.834004	6.488333	-0.028224	3.258736
139.606637	3555.845194	6.493338	-0.028286	3.262220
139.832376	3563.873115	6.498342	-0.028334	3.265704
140.118957	3571.920785	6.503347	-0.028392	3.269195
140.083700	3579.969652	6.508352	-0.028391	3.272670
140.389379	3588.028638	6.513357	-0.028453	3.276159
140.519262	3596.002887	6.518362	-0.028483	3.279601
140.608886	3604.005190	6.523366	-0.028505	3.283050
141.026110	3612.040101	6.528371	-0.028588	3.286522
141.127789	3620.067093	6.533376	-0.028612	3.289975
141.276401	3628.147114	6.538381	-0.028645	3.293448
141.645600	3636.153283	6.543386	-0.028719	3.296895
141.839053	3644.157503	6.548390	-0.028760	3.300330
141.996099	3652.223065	6.553395	-0.028795	3.303787
141.917946	3660.259664	6.558400	-0.028786	3.307219
142.236950	3668.269235	6.563405	-0.028850	3.310650
142.522980	3676.369305	6.568410	-0.028909	3.314116
142.830568	3684.339719	6.573414	-0.028971	3.317523
142.932908	3692.368920	6.578419	-0.028996	3.320944
143.089071	3700.338526	6.583424	-0.029030	3.324338
143.538000	3708.375900	6.588429	-0.029119	3.327769
143.572299	3716.428758	6.593434	-0.029131	3.331187
143.899556	3724.467923	6.598438	-0.029197	3.334606
144.276066	3732.492017	6.603443	-0.029272	3.338018
144.123718	3740.540368	6.608448	-0.029249	3.341416
144.493131	3748.526294	6.613453	-0.029323	3.344804
144.657882	3756.564917	6.618458	-0.029359	3.348204
144.758418	3764.652915	6.623462	-0.029383	3.351618
144.971095	3772.700220	6.628467	-0.029428	3.355016
145.080878	3780.676339	6.633472	-0.029454	3.358376
145.062737	3788.741359	6.638477	-0.029456	3.361766
145.284228	3796.714358	6.643482	-0.029502	3.365122
145.304013	3804.763337	6.648486	-0.029511	3.368500
145.926798	3812.795691	6.653491	-0.029632	3.371889
145.945774	3820.828996	6.658496	-0.029641	3.375253
146.025294	3828.854726	6.663501	-0.029661	3.378613
146.203479	3836.868900	6.668506	-0.029700	3.381968
146.393127	3844.875188	6.673510	-0.029740	3.385317
146.480427	3852.957321	6.678515	-0.029762	3.388691
146.485970	3860.988475	6.683520	-0.029768	3.392037
146.921825	3869.074670	6.688525	-0.029855	3.395418
147.163019	3877.024715	6.693530	-0.029905	3.398732
147.346953	3884.997961	6.698534	-0.029944	3.402050
147.676598	3893.032397	6.703539	-0.030011	3.405396
147.984013	3901.036817	6.708544	-0.030074	3.408725
147.923464	3909.100174	6.713549	-0.030068	3.412062
148.099773	3917.141186	6.718554	-0.030106	3.415395
148.318424	3925.169259	6.723558	-0.030152	3.418721
148.462074	3933.184977	6.728563	-0.030184	3.422036
148.483941	3941.211761	6.733568	-0.030193	3.425348
148.816835	3949.220012	6.738573	-0.030260	3.428660
148.923516	3957.288853	6.743578	-0.030286	3.431986
149.047400	3965.300386	6.748582	-0.030314	3.435286
149.431247	3973.331919	6.753587	-0.030391	3.438599
149.692221	3981.356280	6.758592	-0.030445	3.441902
150.000814	3989.335110	6.763597	-0.030507	3.445185
150.040292	3997.412871	6.768602	-0.030520	3.448496
150.432742	4005.411143	6.773606	-0.030598	3.451783
150.310651	4013.519813	6.778611	-0.030581	3.455095
150.253656	4021.503310	6.783616	-0.030576	3.458355
150.746589	4029.520596	6.788621	-0.030673	3.461644
150.865718	4037.547322	6.793626	-0.030700	3.464921
150.844037	4045.576086	6.798630	-0.030701	3.468192
151.076206	4053.626739	6.803635	-0.030750	3.471476
151.429173	4061.640967	6.808640	-0.030821	3.474746
151.654773	4069.652253	6.813645	-0.030868	3.478008
151.711379	4077.686842	6.818650	-0.030884	3.481271
151.725390	4085.671508	6.823654	-0.030892	3.484509
152.221823	4093.691966	6.828659	-0.030990	3.487774
152.234902	4101.729557	6.833664	-0.030997	3.491027
152.389775	4109.757379	6.838669	-0.031031	3.494278
152.669243	4117.789984	6.843674	-0.031089	3.497532
152.697048	4125.808018	6.848678	-0.031099	3.500769
153.103487	4133.799424	6.853683	-0.031180	3.504004
153.180788	4141.860363	6.858688	-0.031200	3.507254
153.241804	4149.881187	6.863693	-0.031217	3.510484
153.456761	4157.935624	6.868698	-0.031262	3.513729
153.595220	4165.970844	6.873702	-0.031293	3.516961
153.747331	4173.949441	6.878707	-0.031327	3.520168
153.874375	4181.948994	6.883712	-0.031355	3.523380
154.059569	4190.048929	6.888717	-0.031395	3.526630
154.319126	4198.036832	6.893722	-0.031449	3.529836
154.404462	4206.081284	6.898726	-0.031470	3.533055
154.626778	4214.147760	6.903731	-0.031517	3.536284
154.715021	4222.106647	6.908736	-0.031538	3.539464
155.071424	4230.141814	6.913741	-0.031610	3.542679
155.521014	4238.158630	6.918746	-0.031699	3.545886
155.641736	4246.194238	6.923750	-0.031727	3.549089
155.914653	4254.320816	6.928755	-0.031783	3.552329
156.029509	4262.355894	6.933760	-0.031810	3.555525
156.130842	4270.328455	6.938765	-0.031834	3.558693
156.228018	4278.351007	6.943770	-0.031857	3.561877
156.442827	4286.297993	6.948774	-0.031902	3.565033
156.710066	4294.351602	6.953779	-0.031958	3.568229
156.860970	4302.379276	6.958784	-0.031991	3.571409
157.068920	4310.429749	6.963789	-0.032035	3.574596
157.104039	4318.439256	6.968794	-0.032047	3.577760
157.376921	4326.429801	6.973798	-0.032103	3.580920
157.808143	4334.417587	6.978803	-0.032188	3.584081
157.673190	4342.484688	6.983808	-0.032169	3.587254
157.786396	4350.504382	6.988813	-0.032195	3.590412
157.993429	4358.558582	6.993818	-0.032239	3.593584
158.304722	4366.563181	6.998822	-0.032302	3.596737
158.310282	4374.570655	7.003827	-0.032308	3.599879
158.413576	4382.604420	7.008832	-0.032333	3.603031
158.700667	4390.640909	7.013837	-0.032392	3.606188
158.765928	4398.650110	7.018842	-0.032409	3.609324
158.834488	4406.663683	7.023846	-0.032427	3.612459
159.130139	4414.709729	7.028851	-0.032487	3.615611
159.346492	4422.724533	7.033856	-0.032533	3.618745
159.700000	4430.748735	7.038861	-0.032604	3.621885
159.772259	4438.753348	7.043866	-0.032623	3.625006
159.947846	4446.764874	7.048870	-0.032661	3.628130
160.054530	4454.851643	7.053875	-0.032686	3.631278
160.133257	4462.894393	7.058880	-0.032706	3.634406
160.373311	4470.907964	7.063885	-0.032756	3.637524
160.535345	4478.914615	7.068890	-0.032791	3.640635
160.826148	4486.893506	7.073894	-0.032851	3.643736
161.154916	4494.961388	7.078899	-0.032917	3.646869
161.197664	4502.935769	7.083904	-0.032931	3.649956
161.243969	4511.008771	7.088909	-0.032944	3.653079
161.641525	4519.067932	7.093914	-0.033024	3.656203
161.828867	4527.036831	7.098918	-0.033064	3.659284
162.135764	4535.095927	7.103923	-0.033126	3.662400
162.250168	4543.084294	7.108928	-0.033153	3.665481
162.615390	4551.129823	7.113933	-0.033226	3.668588
162.647834	4559.162548	7.118938	-0.033238	3.671679
162.590784	4567.187759	7.123942	-0.033232	3.674762
162.853465	4575.211284	7.128947	-0.033286	3.677850
163.104504	4583.207452	7.133952	-0.033338	3.680924
163.139504	4591.206076	7.138957	-0.033350	3.683992
163.407100	4599.239971	7.143962	-0.033405	3.687076
163.407953	4607.260029	7.148966	-0.033411	3.690145
163.860081	4615.292912	7.153971	-0.033500	3.693229
163.841543	4623.336727	7.158976	-0.033502	3.696302
164.185656	4631.316798	7.163981	-0.033571	3.699357
164.170921	4639.363137	7.168986	-0.033574	3.702426
164.397453	4647.355339	7.173990	-0.033621	3.705478
164.699241	4655.391990	7.178995	-0.033683	3.708546
164.749651	4663.452562	7.184000	-0.033698	3.711614
164.879993	4671.572993	7.189005	-0.033727	3.714704
165.139483	4679.534885	7.194010	-0.033781	3.717735
165.211254	4687.517929	7.199014	-0.033799	3.720767
165.449858	4695.504245	7.204019	-0.033849	3.723801
165.437048	4703.539624	7.209024	-0.033852	3.726846
165.585794	4711.525091	7.214029	-0.033885	3.729873
165.818548	4719.588563	7.219034	-0.033934	3.732929
166.126060	4727.625101	7.224038	-0.033996	3.735974
166.163783	4735.624172	7.229043	-0.034008	3.738997
166.219482	4743.636883	7.234048	-0.034024	3.742022
166.392750	4751.656191	7.239053	-0.034062	3.745050
166.631694	4759.683769	7.244058	-0.034111	3.748080
166.824411	4767.715030	7.249062	-0.034153	3.751108
167.186769	4775.763089	7.254067	-0.034225	3.754144
167.256458	4783.779451	7.259072	-0.034244	3.757159
167.644827	4791.757662	7.264077	-0.034321	3.760164
167.636239	4799.821800	7.269082	-0.034325	3.763190
167.954740	4807.814053	7.274086	-0.034389	3.766194
168.384857	4815.836854	7.279091	-0.034475	3.769209
168.364656	4823.902906	7.284096	-0.034476	3.772228
168.366943	4831.928962	7.289101	-0.034482	3.775230
168.729605	4839.961312	7.294106	-0.034555	3.778240
168.933685	4847.957120	7.299110	-0.034598	3.781231
168.967687	4855.963732	7.304115	-0.034610	3.784219
168.933935	4864.039396	7.309120	-0.034609	3.787230
169.217055	4872.027918	7.314125	-0.034667	3.790212
169.589838	4880.091351	7.319130	-0.034742	3.793222
169.608003	4888.109374	7.324134	-0.034750	3.796205
169.884621	4896.080599	7.329139	-0.034807	3.799174
169.988051	4904.097842	7.334144	-0.034832	3.802153
170.277099	4912.095358	7.339149	-0.034891	3.805127
170.364906	4920.115274	7.344154	-0.034912	3.808103
170.689956	4928.122587	7.349158	-0.034978	3.811076
170.846361	4936.217836	7.354163	-0.035012	3.814077
171.088743	4944.191272	7.359168	-0.035063	3.817031
171.239289	4952.220251	7.364173	-0.035096	3.820002
171.370346	4960.229616	7.369178	-0.035126	3.822963
171.332596	4968.249876	7.374182	-0.035124	3.825922
171.619904	4976.280589	7.379187	-0.035183	3.828890
171.666893	4984.322904	7.384192	-0.035197	3.831854
171.928527	4992.342299	7.389197	-0.035251	3.834812
172.050680	5000.381008	7.394202	-0.035279	3.837772
172.271549	5008.359235	7.399206	-0.035325	3.840710
172.538980	5016.350405	7.404211	-0.035380	3.843651
172.567034	5024.409748	7.409216	-0.035391	3.846609
172.646036	5032.418819	7.414221	-0.035411	3.849548
172.861827	5040.478417	7.419226	-0.035456	3.852506
173.123472	5048.468417	7.424230	-0.035510	3.855438
173.206225	5056.513777	7.429235	-0.035531	3.858383
173.380767	5064.561976	7.434240	-0.035569	3.861329
173.474289	5072.554178	7.439245	-0.035592	3.864251
173.641829	5080.600610	7.444250	-0.035628	3.867192
173.811144	5088.607774	7.449254	-0.035665	3.870117
173.973999	5096.817633	7.454259	-0.035701	3.873113
173.980309	5104.839186	7.459264	-0.035707	3.876034
174.108703	5112.778694	7.464269	-0.035736	3.878927
174.498610	5120.736750	7.469274	-0.035814	3.881829
174.681295	5128.647581	7.474278	-0.035853	3.884707
175.115524	5136.730688	7.479283	-0.035939	3.887651
175.286400	5144.725672	7.484288	-0.035977	3.890555
175.524059	5152.772269	7.489293	-0.036026	3.893477
175.502646	5160.840422	7.494298	-0.036027	3.896400
175.776059	5168.761963	7.499302	-0.036084	3.899273
176.013591	5176.837247	7.504307	-0.036133	3.902199
176.084286	5184.813371	7.509312	-0.036152	3.905084
176.353150	5192.862935	7.514317	-0.036207	3.907997
176.618358	5200.898051	7.519322	-0.036262	3.910902
176.655447	5208.906014	7.524326	-0.036274	3.913791
176.866283	5216.966438	7.529331	-0.036318	3.916700
176.907551	5224.902894	7.534336	-0.036331	3.919560
177.133783	5232.943336	7.539341	-0.036379	3.922457
177.417312	5240.946097	7.544346	-0.036437	3.925341
177.477976	5248.977457	7.549350	-0.036453	3.928228
177.737623	5257.010808	7.554355	-0.036507	3.931117
177.799473	5265.040109	7.559360	-0.036524	3.933999
177.887569	5273.067051	7.564365	-0.036545	3.936879
178.206633	5281.063117	7.569370	-0.036610	3.939750
178.278778	5289.096616	7.574374	-0.036629	3.942627
178.484370	5297.105849	7.579379	-0.036672	3.945496
178.687703	5305.128106	7.584384	-0.036716	3.948368
179.081474	5313.164433	7.589389	-0.036794	3.951246
179.120061	5321.246033	7.594394	-0.036807	3.954132
179.029889	5329.243526	7.599398	-0.036795	3.956983
179.466739	5337.206297	7.604403	-0.036882	3.959829
179.491391	5345.215946	7.609408	-0.036892	3.962682
179.583629	5353.215850	7.614413	-0.036914	3.965532
179.808290	5361.248573	7.619418	-0.036961	3.968393
179.705023	5369.274731	7.624422	-0.036947	3.971244
180.032154	5377.342436	7.629427	-0.037013	3.974115
180.087846	5385.349776	7.634432	-0.037029	3.976958
180.277125	5393.338086	7.639437	-0.037070	3.979794
180.543231	5401.370872	7.644442	-0.037124	3.982645
180.594702	5409.364015	7.649446	-0.037139	3.985477
180.965205	5417.420380	7.654451	-0.037214	3.988334
181.118498	5425.416809	7.659456	-0.037247	3.991165
181.346953	5433.465890	7.664461	-0.037295	3.994013
181.492011	5441.513159	7.669466	-0.037328	3.996857
181.811893	5449.462641	7.674470	-0.037392	3.999667
182.246853	5457.527745	7.679475	-0.037479	4.002518
182.460866	5465.514873	7.684480	-0.037524	4.005336
182.651650	5473.537155	7.689485	-0.037565	4.008164
182.812614	5481.613573	7.694490	-0.037600	4.011009
182.946622	5489.648157	7.699494	-0.037630	4.013836
183.160501	5497.700017	7.704499	-0.037675	4.016668
183.075020	5505.678452	7.709504	-0.037665	4.019469
183.118918	5513.705655	7.714509	-0.037678	4.022286
183.465081	5521.691355	7.719514	-0.037748	4.025091
183.503702	5529.740828	7.724518	-0.037760	4.027912
183.947385	5537.764910	7.729523	-0.037848	4.030729
183.963189	5545.850877	7.734528	-0.037856	4.033558
184.238165	5553.838433	7.739533	-0.037913	4.036355
184.247921	5561.822512	7.744538	-0.037920	4.039145
184.321692	5569.821901	7.749542	-0.037939	4.041939
184.491730	5577.786953	7.754547	-0.037976	4.044721
184.601081	5585.826426	7.759552	-0.038001	4.047526
184.724239	5593.832403	7.764557	-0.038030	4.050317
184.980769	5601.906517	7.769562	-0.038083	4.053132
185.137856	5609.904358	7.774566	-0.038117	4.055917
185.510044	5617.905986	7.779571	-0.038192	4.058705
185.523817	5625.939837	7.784576	-0.038200	4.061497
185.743927	5633.910443	7.789581	-0.038246	4.064267
185.664038	5641.982627	7.794586	-0.038236	4.067067
185.735648	5649.940664	7.799590	-0.038255	4.069828
186.138867	5658.002395	7.804595	-0.038335	4.072627
186.191862	5666.028125	7.809600	-0.038351	4.075407
186.361661	5674.046530	7.814605	-0.038387	4.078184
186.580480	5682.034191	7.819610	-0.038433	4.080949
186.811213	5690.008816	7.824614	-0.038482	4.083708
186.836130	5698.111072	7.829619	-0.038492	4.086506
186.955785	5706.084831	7.834624	-0.038519	4.089259
187.300759	5714.122167	7.839629	-0.038589	4.092036
187.449489	5722.164644	7.844634	-0.038622	4.094809
187.343322	5730.173606	7.849638	-0.038607	4.097566
187.694261	5738.175644	7.854643	-0.038678	4.100325
187.950975	5746.212287	7.859648	-0.038731	4.103092
187.880275	5754.181620	7.864653	-0.038723	4.105830
188.046876	5762.241755	7.869658	-0.038759	4.108601
188.232381	5770.260283	7.874662	-0.038799	4.111355
188.292806	5778.356381	7.879667	-0.038816	4.114133
188.486195	5786.349111	7.884672	-0.038857	4.116875
188.776412	5794.297134	7.889677	-0.038916	4.119601
188.992279	5802.357327	7.894682	-0.038962	4.122363
188.842117	5810.308757	7.899686	-0.038939	4.125081
189.160872	5818.411638	7.904691	-0.039004	4.127855
189.293973	5826.409892	7.909696	-0.039034	4.130588
189.359109	5834.436110	7.914701	-0.039051	4.133329
189.565082	5842.497372	7.919706	-0.039095	4.136082
189.753139	5850.456649	7.924710	-0.039135	4.138798
190.142822	5858.512090	7.929715	-0.039213	4.141547
190.032706	5866.492730	7.934720	-0.039198	4.144263
190.300119	5874.526673	7.939725	-0.039253	4.147000
190.455132	5882.589295	7.944730	-0.039287	4.149743
190.610570	5890.593891	7.949734	-0.039321	4.152465
190.824626	5898.610042	7.954739	-0.039366	4.155189
191.005039	5906.612471	7.959744	-0.039405	4.157907
191.006212	5914.623638	7.964749	-0.039411	4.160624
191.307088	5922.614102	7.969754	-0.039472	4.163335
191.356081	5930.626797	7.974758	-0.039486	4.166049
191.411466	5938.669442	7.979763	-0.039502	4.168772
191.672546	5946.708592	7.984768	-0.039556	4.171494
191.843863	5954.738563	7.989773	-0.039593	4.174210
192.039704	5962.794290	7.994778	-0.039635	4.176934
192.023731	5970.696778	7.999782	-0.039637	4.179601
192.527310	5978.782534	8.004787	-0.039736	4.182334
192.839374	5986.776312	8.009792	-0.039800	4.185033
192.949253	5994.773624	8.014797	-0.039825	4.187728
192.997234	6002.824522	8.019802	-0.039840	4.190439
193.206539	6010.910744	8.024806	-0.039884	4.193162
193.434967	6018.952479	8.029811	-0.039932	4.195869
193.400222	6026.914930	8.034816	-0.039930	4.198544
193.600776	6034.874093	8.039821	-0.039973	4.201219
193.890033	6042.879370	8.044826	-0.040032	4.203909
194.009499	6050.907301	8.049830	-0.040060	4.206602
194.220459	6058.891010	8.054835	-0.040104	4.209280
194.344064	6066.948785	8.059840	-0.040133	4.211981
194.585548	6074.939142	8.064845	-0.040183	4.214658
194.891434	6083.028886	8.069850	-0.040245	4.217367
194.974525	6090.958806	8.074854	-0.040266	4.220019
195.209323	6098.999504	8.079859	-0.040315	4.222708
195.127807	6107.016514	8.084864	-0.040305	4.225383
195.355331	6115.028488	8.089869	-0.040353	4.228059
195.720994	6123.090272	8.094874	-0.040426	4.230751
195.480178	6131.096359	8.099878	-0.040386	4.233416
195.815018	6139.158200	8.104883	-0.040454	4.236104
196.103836	6147.109339	8.109888	-0.040513	4.238753
196.268909	6155.101046	8.114893	-0.040549	4.241413
196.272044	6163.157887	8.119898	-0.040555	4.244091
196.265438	6171.157111	8.124902	-0.040559	4.246748
196.517250	6179.217125	8.129907	-0.040611	4.249426
196.720373	6187.224387	8.134912	-0.040654	4.252085
196.750045	6195.251913	8.139917	-0.040665	4.254746
197.112695	6203.306436	8.144922	-0.040738	4.257419
197.286717	6211.241172	8.149926	-0.040776	4.260048
197.476897	6219.282370	8.154931	-0.040816	4.262710
197.560206	6227.325891	8.159936	-0.040837	4.265371
197.612629	6235.301599	8.164941	-0.040852	4.268008
197.858403	6243.387762	8.169946	-0.040903	4.270681
197.881137	6251.406445	8.174950	-0.040913	4.273328
198.116265	6259.453915	8.179955	-0.040962	4.275985
198.176007	6267.438102	8.184960	-0.040978	4.278618
198.413400	6275.444466	8.189965	-0.041028	4.281258
198.674267	6283.413545	8.194970	-0.041081	4.283884
198.508743	6291.424059	8.199974	-0.041056	4.286518
198.686080	6299.466903	8.204979	-0.041094	4.289165
198.822668	6307.516761	8.209984	-0.041125	4.291812
199.343452	6315.533613	8.214989	-0.041227	4.294449
199.347954	6323.581617	8.219994	-0.041233	4.297091
199.551588	6331.528820	8.224998	-0.041276	4.299700
199.924167	6339.583540	8.230003	-0.041351	4.302344
200.014850	6347.574836	8.235008	-0.041373	4.304963
200.149810	6355.603369	8.240013	-0.041404	4.307593
200.133144	6363.621362	8.245018	-0.041406	4.310216
200.340389	6371.656191	8.250022	-0.041450	4.312846
200.528054	6379.697423	8.255027	-0.041490	4.315475
200.791040	6387.671162	8.260032	-0.041544	4.318082
200.940866	6395.688766	8.265037	-0.041577	4.320700
201.066955	6403.691737	8.270042	-0.041606	4.323312
201.252688	6411.704973	8.275046	-0.041646	4.325926
201.503735	6419.747563	8.280051	-0.041698	4.328549
201.579885	6427.748168	8.285056	-0.041717	4.331155
201.939235	6435.809815	8.290061	-0.041790	4.333781
202.194601	6443.846112	8.295066	-0.041843	4.336397
202.035014	6451.769454	8.300070	-0.041818	4.338971
202.093191	6459.860085	8.305075	-0.041834	4.341600
202.292368	6467.816090	8.310080	-0.041877	4.344184
202.654515	6475.845704	8.315085	-0.041949	4.346792
202.705241	6483.876140	8.320090	-0.041964	4.349396
202.682221	6491.916781	8.325094	-0.041965	4.352002
203.047548	6499.999681	8.330099	-0.042038	4.354622
203.227819	6507.975544	8.335104	-0.042077	4.357205
203.363783	6515.933932	8.340109	-0.042108	4.359780
203.424100	6523.971025	8.345114	-0.042124	4.362379
203.534666	6531.884379	8.350118	-0.042150	4.364937
203.882054	6539.976767	8.355123	-0.042220	4.367552
204.174438	6547.975531	8.360128	-0.042280	4.370135
204.337972	6555.995148	8.365133	-0.042316	4.372723
204.540044	6564.081841	8.370138	-0.042358	4.375330
204.491360	6572.082121	8.375142	-0.042355	4.377907
204.819660	6580.048179	8.380147	-0.042421	4.380474
204.829241	6588.055890	8.385152	-0.042428	4.383050
205.122906	6596.059339	8.390157	-0.042488	4.385626
205.307990	6604.157003	8.395162	-0.042528	4.388229
205.306286	6612.148104	8.400166	-0.042533	4.390796
205.487950	6620.152378	8.405171	-0.042572	4.393366
205.601854	6628.167450	8.410176	-0.042598	4.395938
206.160012	6636.202130	8.415181	-0.042708	4.398517
206.324857	6644.206449	8.420186	-0.042744	4.401083
206.482640	6652.177597	8.425190	-0.042778	4.403636
206.593730	6660.225437	8.430195	-0.042804	4.406213
206.921302	6668.279416	8.435200	-0.042871	4.408790
206.853897	6676.291814	8.440205	-0.042863	4.411351
207.160217	6684.332265	8.445210	-0.042926	4.413922
207.448470	6692.347496	8.450214	-0.042985	4.416482
207.532104	6700.320745	8.455219	-0.043005	4.419027
207.775435	6708.400975	8.460224	-0.043056	4.421605
207.861198	6716.342406	8.465229	-0.043077	4.424137
208.298653	6724.439087	8.470234	-0.043164	4.426718
208.133709	6732.407259	8.475238	-0.043138	4.429254
208.238428	6740.479101	8.480243	-0.043163	4.431823
208.356397	6748.500492	8.485248	-0.043191	4.434374
208.435802	6756.491724	8.490253	-0.043211	4.436914
208.951267	6764.501196	8.495258	-0.043312	4.439461
208.869430	6772.527574	8.500262	-0.043302	4.442008
209.126397	6780.469320	8.505267	-0.043355	4.444529
209.180999	6788.533602	8.510272	-0.043370	4.447086
209.249076	6796.520586	8.515277	-0.043388	4.449618
209.726458	6804.594636	8.520282	-0.043483	4.452177
209.593212	6812.570778	8.525286	-0.043463	4.454701
209.631720	6820.607495	8.530291	-0.043476	4.457243
209.959562	6828.644277	8.535296	-0.043542	4.459786
209.843868	6836.598253	8.540301	-0.043526	4.462298
210.056673	6844.620002	8.545306	-0.043570	4.464833
210.011940	6852.621716	8.550310	-0.043567	4.467358
210.349591	6860.640369	8.555315	-0.043636	4.469889
210.438762	6868.730911	8.560320	-0.043657	4.472440
210.400058	6876.716532	8.565325	-0.043656	4.474956
210.630677	6884.761212	8.570330	-0.043704	4.477490
210.657433	6892.689700	8.575335	-0.043714	4.479985
211.005944	6900.719504	8.580339	-0.043784	4.482512
211.211519	6908.703810	8.585344	-0.043828	4.485023
211.219978	6916.800039	8.590349	-0.043835	4.487567
211.280085	6924.795936	8.595354	-0.043851	4.490078
211.695346	6932.826702	8.600359	-0.043934	4.492599
211.718054	6940.848986	8.605363	-0.043943	4.495116
211.637363	6948.869778	8.610368	-0.043933	4.497630
211.577171	6956.827069	8.615373	-0.043927	4.500123
212.057635	6964.911545	8.620378	-0.044022	4.502656
212.002327	6972.835850	8.625383	-0.044017	4.505135
212.062924	6980.916267	8.630387	-0.044034	4.507663
212.371878	6988.960202	8.635392	-0.044097	4.510178
212.497246	6996.993274	8.640397	-0.044125	4.512689
212.617622	7005.097922	8.645402	-0.044153	4.515220
212.542383	7012.990560	8.650407	-0.044144	4.517682
212.950302	7020.940862	8.655411	-0.044225	4.520163
213.206067	7028.994004	8.660416	-0.044278	4.522674
213.341809	7036.937331	8.665421	-0.044309	4.525149
213.493703	7045.056448	8.670426	-0.044342	4.527678
213.721745	7053.014080	8.675431	-0.044390	4.530155
213.735775	7061.083010	8.680435	-0.044398	4.532665
214.052134	7069.092188	8.685440	-0.044462	4.535155
213.892282	7077.109892	8.690445	-0.044438	4.537646
214.260471	7085.071414	8.695450	-0.044512	4.540119
214.284354	7093.109890	8.700455	-0.044521	4.542614
214.622074	7101.138935	8.705459	-0.044590	4.545105
214.534881	7109.175868	8.710464	-0.044579	4.547596
214.722499	7117.148196	8.715469	-0.044619	4.550066
215.302297	7125.205630	8.720474	-0.044732	4.552562
215.263231	7133.205172	8.725479	-0.044730	4.555038
215.517682	7141.289452	8.730483	-0.044783	4.557539
215.615622	7149.217366	8.735488	-0.044806	4.559990
215.801988	7157.255331	8.740493	-0.044846	4.562474
215.880370	7165.239550	8.745498	-0.044866	4.564940
216.046452	7173.257122	8.750503	-0.044902	4.567415
216.399905	7181.289550	8.755507	-0.044973	4.569893
216.542253	7189.329258	8.760512	-0.045005	4.572372
216.548662	7197.330270	8.765517	-0.045012	4.574837
216.747812	7205.405981	8.770522	-0.045054	4.577325
216.719329	7213.345821	8.775527	-0.045054	4.579769
216.918132	7221.378598	8.780531	-0.045096	4.582240
217.078890	7229.390504	8.785536	-0.045131	4.584703
217.089561	7237.416293	8.790541	-0.045139	4.587170
217.402889	7245.452870	8.795546	-0.045202	4.589638
217.392765	7253.484374	8.800551	-0.045206	4.592104
217.668149	7261.523758	8.805555	-0.045262	4.594571
217.813802	7269.554545	8.810560	-0.045295	4.597033
217.885416	7277.466514	8.815565	-0.045313	4.599458
218.228677	7285.574031	8.820570	-0.045383	4.601942
218.233346	7293.473222	8.825575	-0.045389	4.604360
218.345399	7301.553049	8.830579	-0.045415	4.606832
218.648435	7309.573838	8.835584	-0.045477	4.609285
218.804117	7317.628719	8.840589	-0.045511	4.611747
218.967075	7325.648103	8.845594	-0.045546	4.614197
218.840198	7333.653422	8.850599	-0.045528	4.616641
219.164346	7341.630264	8.855603	-0.045594	4.619075
219.263086	7349.651301	8.860608	-0.045617	4.621522
219.336378	7357.615154	8.865613	-0.045636	4.623950
219.569889	7365.686869	8.870618	-0.045685	4.626409
219.817358	7373.685052	8.875623	-0.045736	4.628844
220.060606	7381.691650	8.880627	-0.045787	4.631281
220.041619	7389.785376	8.885632	-0.045789	4.633743
220.070215	7397.779737	8.890637	-0.045799	4.636173
220.361045	7405.762317	8.895642	-0.045859	4.638599
220.605837	7413.747052	8.900647	-0.045910	4.641024
220.680177	7421.793319	8.905651	-0.045929	4.643466
220.817345	7429.800772	8.910656	-0.045960	4.645895
220.891482	7437.792752	8.915661	-0.045979	4.648319
221.269033	7445.811392	8.920666	-0.046054	4.650749
220.980143	7453.832462	8.925671	-0.046006	4.653178
220.996976	7461.879190	8.930675	-0.046014	4.655614
221.262652	7469.892774	8.935680	-0.046069	4.658039
221.418888	7477.856571	8.940685	-0.046103	4.660447
221.636167	7485.895032	8.945690	-0.046149	4.662877
221.696388	7493.895825	8.950695	-0.046165	4.665294
221.932041	7501.924261	8.955699	-0.046215	4.667718
221.969191	7509.981997	8.960704	-0.046227	4.670150
222.176969	7518.010547	8.965709	-0.046271	4.672571
222.288428	7526.110233	8.970714	-0.046297	4.675013
222.398812	7534.068071	8.975719	-0.046323	4.677410
222.404192	7541.966264	8.980723	-0.046329	4.679789
222.733036	7550.091147	8.985728	-0.046395	4.682234
222.820902	7557.992826	8.990733	-0.046417	4.684611
222.990781	7566.055837	8.995738	-0.046454	4.687036
222.968342	7574.043012	9.000743	-0.046455	4.689436
223.306278	7582.092577	9.005747	-0.046523	4.691853
223.497940	7590.107041	9.010752	-0.046564	4.694259
223.341141	7598.098500	9.015757	-0.046540	4.696658
223.725909	7606.136075	9.020762	-0.046617	4.699067
223.683041	7614.136494	9.025767	-0.046615	4.701466
223.837489	7622.124644	9.030771	-0.046649	4.703859
224.010449	7630.168161	9.035776	-0.046686	4.706267
224.182634	7638.163698	9.040781	-0.046723	4.708660
224.395235	7646.213789	9.045786	-0.046768	4.711067
224.266407	7654.222623	9.050791	-0.046750	4.713462
224.619543	7662.270662	9.055795	-0.046821	4.715867
224.850527	7670.270730	9.060800	-0.046869	4.718256
224.913457	7678.253675	9.065805	-0.046886	4.720639
225.096088	7686.296128	9.070810	-0.046925	4.723038
225.174623	7694.266449	9.075815	-0.046945	4.725415
225.241809	7702.358056	9.080819	-0.046963	4.727826
225.380134	7710.356995	9.085824	-0.046994	4.730209
225.334143	7718.381386	9.090829	-0.046991	4.732599
225.534541	7726.437345	9.095834	-0.047033	4.734996
225.624877	7734.374630	9.100839	-0.047055	4.737357
225.875549	7742.311200	9.105843	-0.047107	4.739716
226.144064	7750.471633	9.110848	-0.047163	4.742140
225.975108	7758.358500	9.115853	-0.047136	4.744483
226.358382	7766.508498	9.120858	-0.047213	4.746901
226.488280	7774.467508	9.125863	-0.047242	4.749262
226.631500	7782.474906	9.130867	-0.047274	4.751637
226.750709	7790.546157	9.135872	-0.047302	4.754029
226.957417	7798.543458	9.140877	-0.047346	4.756397
227.298854	7806.535828	9.145882	-0.047415	4.758763
227.394330	7814.538948	9.150887	-0.047438	4.761131
227.536304	7822.498088	9.155891	-0.047469	4.763485
227.742086	7830.572891	9.160896	-0.047513	4.765872
227.879235	7838.548492	9.165901	-0.047544	4.768229
228.082677	7846.595526	9.170906	-0.047587	4.770605
228.076686	7854.658825	9.175911	-0.047591	4.772985
228.247613	7862.661750	9.180915	-0.047628	4.775346
228.407128	7870.684442	9.185920	-0.047663	4.777712
228.603305	7878.606789	9.190925	-0.047705	4.780046
228.945638	7886.724765	9.195930	-0.047774	4.782437
228.834202	7894.629757	9.200935	-0.047758	4.784765
229.210324	7902.750041	9.205939	-0.047834	4.787154
229.344374	7910.735283	9.210944	-0.047864	4.789502
229.226620	7918.753858	9.215949	-0.047847	4.791861
229.504760	7926.776720	9.220954	-0.047904	4.794218
229.809557	7934.788088	9.225959	-0.047967	4.796570
229.833235	7942.742995	9.230963	-0.047976	4.798905
229.921150	7950.787882	9.235968	-0.047998	4.801266
229.930568	7958.767445	9.240973	-0.048005	4.803606
230.195154	7966.830450	9.245978	-0.048059	4.805969
230.164235	7974.830069	9.250983	-0.048059	4.808313
230.280114	7982.849756	9.255987	-0.048086	4.810662
230.528883	7990.401916	9.260992	-0.048137	4.812872
230.615399	7995.051503	9.265997	-0.048156	4.814232

230.743071	7997.680695	9.271002	-0.048182	4.815001
230.973844	7999.124084	9.276007	-0.048226	4.815422
231.141607	7999.602801	9.281011	-0.048257	4.815561
230.929334	8000.351839	9.286016	-0.048218	4.815781
230.841796	8000.515868	9.291021	-0.048202	4.815829
231.259751	8000.538636	9.296026	-0.048280	4.815834
231.110001	8000.505268	9.301031	-0.048252	4.815825
231.137506	8000.539872	9.306035	-0.048258	4.815835
231.160547	8000.435649	9.311040	-0.048262	4.815804
231.179988	8000.513885	9.316045	-0.048266	4.815827
231.122567	8000.546050	9.321050	-0.048255	4.815837
231.350056	8000.502767	9.326055	-0.048297	4.815823
231.480852	8000.532637	9.331059	-0.048322	4.815831
231.418034	8000.445170	9.336064	-0.048310	4.815806
231.453901	8000.501257	9.341069	-0.048317	4.815822
231.627791	8000.539296	9.346074	-0.048349	4.815833
231.401467	8000.504689	9.351079	-0.048307	4.815823
231.394090	8000.445870	9.356083	-0.048306	4.815806
231.584840	8000.554627	9.361088	-0.048341	4.815837
231.599954	8000.521787	9.366093	-0.048344	4.815828
231.720215	8000.440481	9.371098	-0.048367	4.815803
231.671069	8000.526148	9.376103	-0.048358	4.815828
231.780339	8000.546065	9.381107	-0.048378	4.815834
231.952555	8000.478406	9.386112	-0.048410	4.815813
231.809523	8000.516660	9.391117	-0.048384	4.815825
231.889509	8000.549979	9.396122	-0.048399	4.815834
231.760256	8000.491324	9.401127	-0.048375	4.815818
231.784386	8000.457563	9.406131	-0.048379	4.815808
232.044060	8000.507661	9.411136	-0.048427	4.815821
232.051307	8000.499244	9.416141	-0.048429	4.815819
232.037681	8000.556667	9.421146	-0.048426	4.815836
232.002609	8000.438694	9.426151	-0.048420	4.815801
231.990292	8000.526025	9.431155	-0.048418	4.815827
232.042688	8000.530079	9.436160	-0.048428	4.815828
232.014586	8000.516821	9.441165	-0.048422	4.815824
232.276920	8000.540279	9.446170	-0.048471	4.815830
232.277989	8000.463450	9.451175	-0.048471	4.815807
232.188851	8000.552741	9.456179	-0.048455	4.815834
232.281867	8000.470994	9.461184	-0.048472	4.815809
232.262732	8000.530463	9.466189	-0.048469	4.815827
232.199383	8000.467535	9.471194	-0.048457	4.815809
232.230036	8000.508596	9.476199	-0.048463	4.815821
232.369372	8000.538606	9.481203	-0.048489	4.815829
232.256960	8000.488761	9.486208	-0.048468	4.815815
232.157056	8000.533048	9.491213	-0.048449	4.815828
232.296294	8000.471261	9.496218	-0.048475	4.815809
232.271523	8000.501819	9.501223	-0.048471	4.815818
232.193010	8000.527240	9.506227	-0.048456	4.815826
232.416711	8000.473222	9.511232	-0.048498	4.815809
232.335863	8000.537030	9.516237	-0.048483	4.815828
232.280351	8000.540407	9.521242	-0.048473	4.815830
232.157614	8000.521350	9.526247	-0.048450	4.815825
232.469104	8000.505043	9.531251	-0.048508	4.815818
232.357400	8000.492568	9.536256	-0.048487	4.815815
232.240040	8000.486406	9.541261	-0.048465	4.815814
232.420389	8000.445563	9.546266	-0.048499	4.815801
232.539888	8000.514746	9.551271	-0.048521	4.815821
232.298093	8000.454270	9.556275	-0.048476	4.815804
232.365411	8000.543956	9.561280	-0.048489	4.815830
232.418742	8000.438085	9.566285	-0.048499	4.815799
232.480248	8000.563968	9.571290	-0.048511	4.815836
232.398674	8000.498611	9.576295	-0.048495	4.815817
232.375646	8000.524928	9.581299	-0.048491	4.815825
232.508631	8000.453433	9.586304	-0.048516	4.815803
232.432869	8000.501313	9.591309	-0.048502	4.815818
232.549653	8000.529891	9.596314	-0.048524	4.815825
232.542965	8000.536192	9.601319	-0.048523	4.815827
232.356068	8000.524636	9.606323	-0.048488	4.815825
232.668164	8000.507271	9.611328	-0.048546	4.815818
232.678994	8000.493575	9.616333	-0.048548	4.815814
232.690490	8000.528990	9.621338	-0.048550	4.815824
232.643225	8000.443907	9.626343	-0.048541	4.815800
232.791375	8000.530631	9.631347	-0.048569	4.815824
232.823061	8000.546092	9.636352	-0.048575	4.815829
232.584167	8000.495268	9.641357	-0.048531	4.815815
232.655201	8000.518837	9.646362	-0.048544	4.815822
232.765567	8000.502481	9.651367	-0.048565	4.815816
232.547200	8000.492551	9.656371	-0.048524	4.815814
232.645550	8000.518696	9.661376	-0.048542	4.815822
232.786398	8000.498563	9.666381	-0.048569	4.815815
232.754433	8000.510859	9.671386	-0.048563	4.815819
232.559654	8000.490637	9.676391	-0.048526	4.815814
232.647806	8000.526223	9.681395	-0.048543	4.815824
232.891481	8000.529101	9.686400	-0.048588	4.815823
232.751535	8000.419036	9.691405	-0.048562	4.815792
232.821222	8000.527974	9.696410	-0.048575	4.815823
232.807509	8000.505342	9.701415	-0.048573	4.815817
232.720209	8000.541294	9.706419	-0.048557	4.815828
232.750858	8000.523649	9.711424	-0.048562	4.815823
232.881388	8000.517225	9.716429	-0.048587	4.815820
233.080824	8000.479894	9.721434	-0.048624	4.815808
232.867816	8000.480724	9.726439	-0.048584	4.815809
232.915396	8000.528464	9.731443	-0.048593	4.815823
232.965210	8000.559162	9.736448	-0.048603	4.815832
232.824779	8000.453358	9.741453	-0.048577	4.815802
232.955568	8000.575026	9.746458	-0.048601	4.815837
232.948706	8000.473517	9.751463	-0.048600	4.815807
233.015231	8000.557855	9.756467	-0.048612	4.815831
233.079917	8000.538625	9.761472	-0.048624	4.815825
233.001044	8000.427413	9.766477	-0.048610	4.815793
233.212382	8000.567463	9.771482	-0.048649	4.815833
232.878284	8000.463864	9.776487	-0.048587	4.815804
232.843748	8000.544432	9.781491	-0.048581	4.815828
233.207880	8000.533247	9.786496	-0.048648	4.815823
233.028864	8000.515413	9.791501	-0.048615	4.815819
233.006397	8000.448876	9.796506	-0.048611	4.815799
233.262037	8000.543744	9.801511	-0.048659	4.815826
233.084993	8000.426674	9.806515	-0.048626	4.815793
233.245093	8000.557357	9.811520	-0.048656	4.815830
233.061643	8000.534114	9.816525	-0.048622	4.815824
233.066072	8000.455202	9.821530	-0.048622	4.815801
233.285197	8000.548413	9.826535	-0.048663	4.815827
233.189873	8000.534067	9.831539	-0.048646	4.815823
233.425722	8000.452494	9.836544	-0.048689	4.815798
233.139767	8000.501244	9.841549	-0.048636	4.815814
233.053908	8000.552164	9.846554	-0.048620	4.815829
233.207297	8000.467122	9.851559	-0.048649	4.815804
233.341574	8000.535478	9.856563	-0.048674	4.815823
233.034564	8000.551865	9.861568	-0.048617	4.815829
233.160222	8000.522948	9.866573	-0.048640	4.815820
233.493841	8000.524079	9.871578	-0.048703	4.815819
233.540650	8000.433043	9.876583	-0.048711	4.815792
233.327456	8000.554487	9.881587	-0.048672	4.815829
233.390218	8000.441294	9.886592	-0.048683	4.815795
233.187607	8000.518078	9.891597	-0.048646	4.815819
233.411436	8000.539849	9.896602	-0.048688	4.815824
233.380418	8000.513734	9.901607	-0.048682	4.815817
233.119193	8000.525525	9.906611	-0.048633	4.815821
233.174374	8000.527490	9.911616	-0.048644	4.815822
233.161644	8000.500604	9.916621	-0.048641	4.815814
233.271954	8000.440483	9.921626	-0.048662	4.815796
233.314958	8000.545789	9.926631	-0.048670	4.815826
233.353825	8000.545355	9.931635	-0.048677	4.815826
233.395896	8000.453176	9.936640	-0.048685	4.815799
233.196197	8000.506524	9.941645	-0.048648	4.815815
233.296417	8000.551913	9.946650	-0.048667	4.815828
233.381155	8000.477503	9.951655	-0.048682	4.815806
233.316527	8000.540507	9.956659	-0.048671	4.815825
233.416822	8000.415112	9.961664	-0.048689	4.815788
233.443486	8000.473188	9.966669	-0.048694	4.815804
233.382936	8000.493562	9.971674	-0.048683	4.815811
233.309288	8000.483836	9.976679	-0.048669	4.815808
233.360222	8000.554047	9.981683	-0.048679	4.815828
233.396387	8000.524749	9.986688	-0.048686	4.815820
233.326474	8000.518286	9.991693	-0.048673	4.815818
233.450089	8000.534167	9.996698	-0.048696	4.815822
233.400811	8000.492813	10.001703	-0.048687	4.815810
233.497682	8000.447418	10.006707	-0.048705	4.815797
233.561501	8000.541320	10.011712	-0.048717	4.815824
233.604230	8000.477971	10.016717	-0.048725	4.815805
233.549918	8000.370357	10.021722	-0.048715	4.815774
233.387019	8000.553457	10.026727	-0.048684	4.815828
233.393582	8000.486321	10.031731	-0.048686	4.815808
233.647799	8000.560887	10.036736	-0.048733	4.815829
233.506492	8000.495628	10.041741	-0.048707	4.815811
233.425591	8000.439887	10.046746	-0.048692	4.815795
233.545007	8000.562441	10.051751	-0.048714	4.815830
233.719611	8000.456393	10.056755	-0.048747	4.815798
233.667153	8000.552685	10.061760	-0.048737	4.815827
233.530666	8000.517392	10.066765	-0.048712	4.815817
233.573171	8000.465781	10.071770	-0.048720	4.815802
233.641357	8000.464754	10.076775	-0.048732	4.815801
233.514017	8000.555564	10.081779	-0.048709	4.815828
233.389165	8000.467089	10.086784	-0.048685	4.815803
233.573950	8000.521319	10.091789	-0.048720	4.815818
233.768460	8000.551155	10.096794	-0.048756	4.815826
233.702551	8000.486049	10.101799	-0.048744	4.815807
233.750229	8000.528454	10.106803	-0.048753	4.815819
233.875591	8000.546499	10.111808	-0.048776	4.815824
233.836234	8000.514911	10.116813	-0.048769	4.815815
233.922200	8000.546195	10.121818	-0.048785	4.815823
233.699406	8000.446528	10.126823	-0.048744	4.815795
233.722268	8000.557914	10.131827	-0.048748	4.815828
233.544360	8000.463243	10.136832	-0.048715	4.815801
233.644165	8000.544919	10.141837	-0.048734	4.815824
233.737754	8000.419415	10.146842	-0.048751	4.815787
233.520698	8000.573886	10.151847	-0.048711	4.815833
233.749417	8000.470849	10.156851	-0.048753	4.815802
233.745733	8000.471862	10.161856	-0.048753	4.815803
233.500118	8000.537276	10.166861	-0.048707	4.815823
233.470660	8000.469557	10.171866	-0.048702	4.815803
233.757515	8000.470999	10.176871	-0.048755	4.815802
233.625972	8000.535057	10.181875	-0.048731	4.815822
233.564783	8000.573566	10.186880	-0.048719	4.815833
233.562521	8000.460388	10.191885	-0.048719	4.815800
233.689441	8000.549974	10.196890	-0.048743	4.815826
233.744145	8000.455864	10.201895	-0.048753	4.815798
233.687230	8000.545679	10.206899	-0.048742	4.815824
233.799980	8000.462114	10.211904	-0.048763	4.815799
233.837890	8000.533182	10.216909	-0.048771	4.815820
233.944907	8000.553064	10.221914	-0.048791	4.815825
233.702581	8000.524598	10.226919	-0.048745	4.815818
233.784336	8000.464015	10.231923	-0.048761	4.815800
233.654624	8000.566529	10.236928	-0.048737	4.815831
233.682297	8000.455970	10.241933	-0.048742	4.815798
233.803457	8000.484620	10.246938	-0.048764	4.815806
233.671271	8000.537992	10.251943	-0.048740	4.815822
233.565135	8000.521336	10.256947	-0.048720	4.815818
233.786621	8000.538800	10.261952	-0.048761	4.815822
233.653397	8000.514234	10.266957	-0.048737	4.815815
233.612256	8000.468742	10.271962	-0.048729	4.815802
233.813271	8000.541381	10.276967	-0.048767	4.815823
233.804715	8000.549787	10.281971	-0.048765	4.815825
233.657925	8000.471630	10.286976	-0.048738	4.815803
233.655502	8000.456652	10.291981	-0.048737	4.815798
233.705718	8000.567414	10.296986	-0.048747	4.815831
233.715510	8000.483251	10.301991	-0.048749	4.815806
233.808512	8000.540266	10.306995	-0.048766	4.815822
233.782552	8000.393614	10.312000	-0.048761	4.815779
233.690171	8000.549035	10.317005	-0.048744	4.815825
233.784557	8000.442758	10.322010	-0.048762	4.815794
233.676512	8000.477307	10.327015	-0.048742	4.815804
233.554318	8000.520167	10.332019	-0.048719	4.815818
233.499371	8000.504339	10.337024	-0.048709	4.815813
233.729947	8000.536894	10.342029	-0.048752	4.815822
233.664836	8000.468598	10.347034	-0.048740	4.815802
233.716095	8000.550556	10.352039	-0.048749	4.815826
233.941547	8000.452803	10.357043	-0.048791	4.815796
234.016450	8000.486042	10.362048	-0.048805	4.815805
233.899039	8000.562070	10.367053	-0.048784	4.815828
233.973646	8000.455472	10.372058	-0.048797	4.815797
234.034984	8000.539728	10.377063	-0.048809	4.815821
234.005698	8000.437854	10.382067	-0.048804	4.815791
233.957768	8000.542758	10.387072	-0.048795	4.815822
233.871392	8000.531759	10.392077	-0.048779	4.815819
233.905114	8000.541916	10.397082	-0.048785	4.815822
233.883302	8000.452972	10.402087	-0.048781	4.815796
233.832749	8000.558901	10.407091	-0.048772	4.815828
233.819787	8000.463696	10.412096	-0.048769	4.815800
233.688802	8000.525627	10.417101	-0.048745	4.815818
233.958607	8000.563087	10.422106	-0.048795	4.815828
233.839039	8000.506719	10.427111	-0.048773	4.815812
233.793774	8000.516666	10.432115	-0.048765	4.815815
233.980795	8000.463122	10.437120	-0.048800	4.815799
233.927839	8000.507102	10.442125	-0.048790	4.815812
233.996830	8000.538111	10.447130	-0.048803	4.815821
233.887528	8000.520336	10.452135	-0.048782	4.815816
234.041126	8000.517489	10.457139	-0.048811	4.815814
234.153670	8000.462741	10.462144	-0.048832	4.815798
233.842537	8000.527095	10.467149	-0.048774	4.815818
234.079872	8000.462624	10.472154	-0.048818	4.815798
234.206888	8000.531932	10.477159	-0.048842	4.815818
234.121437	8000.511341	10.482163	-0.048826	4.815812
234.133588	8000.539295	10.487168	-0.048829	4.815820
233.989990	8000.536977	10.492173	-0.048802	4.815820
233.906088	8000.463040	10.497178	-0.048786	4.815799
234.157621	8000.473518	10.502183	-0.048833	4.815801
233.882232	8000.460529	10.507187	-0.048782	4.815798
234.067139	8000.501952	10.512192	-0.048816	4.815810
233.942625	8000.556516	10.517197	-0.048793	4.815826
234.021831	8000.475610	10.522202	-0.048808	4.815802
234.132770	8000.475275	10.527207	-0.048829	4.815802
233.987388	8000.548716	10.532211	-0.048802	4.815824
233.951523	8000.470218	10.537216	-0.048795	4.815801
233.950497	8000.453127	10.542221	-0.048795	4.815796
233.991318	8000.470871	10.547226	-0.048803	4.815801
234.159321	8000.469324	10.552231	-0.048834	4.815800
233.814105	8000.450936	10.557235	-0.048770	4.815796
234.066489	8000.547890	10.562240	-0.048817	4.815823
233.995633	8000.526467	10.567245	-0.048804	4.815817
233.839027	8000.550624	10.572250	-0.048775	4.815825
233.995967	8000.483785	10.577255	-0.048804	4.815805
233.976764	8000.487749	10.582259	-0.048800	4.815806
233.842560	8000.533617	10.587264	-0.048776	4.815820
233.844565	8000.511238	10.592269	-0.048776	4.815813
233.980855	8000.535864	10.597274	-0.048801	4.815820
233.914508	8000.453671	10.602279	-0.048789	4.815796
233.953605	8000.537568	10.607283	-0.048796	4.815821
233.949670	8000.490542	10.612288	-0.048796	4.815807
233.970844	8000.537856	10.617293	-0.048800	4.815821
233.938598	8000.525598	10.622298	-0.048794	4.815817
234.126697	8000.463532	10.627303	-0.048829	4.815798
234.167672	8000.452458	10.632307	-0.048837	4.815795
234.219118	8000.495993	10.637312	-0.048846	4.815807
234.063725	8000.532979	10.642317	-0.048817	4.815819
233.964744	8000.463067	10.647322	-0.048799	4.815799
234.013346	8000.555657	10.652327	-0.048808	4.815826
233.920459	8000.496518	10.657331	-0.048791	4.815809
234.041753	8000.501687	10.662336	-0.048813	4.815810
234.095223	8000.483343	10.667341	-0.048823	4.815804
234.072539	8000.478711	10.672346	-0.048819	4.815803
234.009220	8000.474490	10.677351	-0.048808	4.815802
234.213577	8000.475666	10.682355	-0.048846	4.815801
234.205626	8000.341046	10.687360	-0.048844	4.815762
234.096179	8000.394787	10.692365	-0.048824	4.815778
234.081579	8000.490624	10.697370	-0.048821	4.815806
234.221255	8000.386145	10.702375	-0.048847	4.815775
234.087610	8000.556912	10.707379	-0.048823	4.815826
234.022715	8000.479012	10.712384	-0.048810	4.815803
234.010380	8000.511907	10.717389	-0.048808	4.815813
233.927331	8000.463602	10.722394	-0.048793	4.815799
234.014487	8000.551478	10.727399	-0.048809	4.815824
234.241226	8000.445206	10.732403	-0.048851	4.815792
234.260496	8000.557603	10.737408	-0.048855	4.815825
234.049243	8000.521100	10.742413	-0.048816	4.815815
234.292109	8000.463123	10.747418	-0.048861	4.815797
234.148546	8000.548335	10.752423	-0.048834	4.815823
234.128129	8000.457277	10.757427	-0.048831	4.815796
234.173861	8000.561563	10.762432	-0.048839	4.815827
234.298852	8000.453645	10.767437	-0.048862	4.815794
234.126394	8000.486085	10.772442	-0.048830	4.815805
234.092834	8000.474872	10.777447	-0.048824	4.815802
234.175331	8000.546662	10.782451	-0.048840	4.815822
234.074554	8000.473519	10.787456	-0.048821	4.815801
234.053173	8000.493459	10.792461	-0.048817	4.815807
234.139490	8000.379578	10.797466	-0.048833	4.815774
234.292071	8000.450367	10.802471	-0.048862	4.815793
234.281221	8000.507837	10.807475	-0.048860	4.815810
234.053453	8000.474269	10.812480	-0.048817	4.815802
234.029171	8000.454667	10.817485	-0.048813	4.815796
234.073642	8000.560000	10.822490	-0.048821	4.815827
233.889057	8000.471624	10.827495	-0.048787	4.815802
233.894191	8000.543230	10.832499	-0.048788	4.815823
234.129632	8000.465919	10.837504	-0.048832	4.815799
234.063671	8000.542779	10.842509	-0.048820	4.815822
234.092239	8000.461054	10.847514	-0.048825	4.815798
234.055039	8000.546919	10.852519	-0.048818	4.815823
233.948888	8000.527060	10.857523	-0.048798	4.815818
234.030868	8000.409907	10.862528	-0.048814	4.815783
234.307742	8000.478437	10.867533	-0.048865	4.815802
234.405538	8000.557947	10.872538	-0.048884	4.815824
234.352472	8000.461024	10.877543	-0.048874	4.815796
234.102827	8000.540249	10.882547	-0.048827	4.815821
234.397551	8000.486314	10.887552	-0.048882	4.815803
234.143299	8000.541981	10.892557	-0.048835	4.815821
234.026568	8000.453636	10.897562	-0.048813	4.815796
234.179748	8000.540446	10.902567	-0.048842	4.815820
234.126006	8000.532109	10.907571	-0.048832	4.815818
234.130237	8000.472406	10.912576	-0.048833	4.815801
234.217233	8000.546404	10.917581	-0.048849	4.815822
234.202048	8000.465038	10.922586	-0.048846	4.815798
234.223334	8000.532636	10.927591	-0.048850	4.815818
234.142407	8000.529196	10.932595	-0.048835	4.815817
234.285695	8000.470676	10.937600	-0.048862	4.815799
234.137237	8000.539797	10.942605	-0.048834	4.815820
234.382913	8000.472259	10.947610	-0.048880	4.815799
234.422245	8000.481439	10.952615	-0.048888	4.815802
234.542641	8000.541034	10.957619	-0.048910	4.815819
234.539470	8000.403288	10.962624	-0.048909	4.815779
234.311867	8000.487140	10.967629	-0.048867	4.815804
234.491169	8000.535946	10.972634	-0.048901	4.815818
234.350427	8000.481369	10.977639	-0.048874	4.815802
234.138512	8000.469406	10.982643	-0.048835	4.815800
234.238721	8000.450751	10.987648	-0.048854	4.815794
234.412263	8000.438619	10.992653	-0.048886	4.815789
234.331833	8000.390356	10.997658	-0.048871	4.815776
234.460421	8000.407385	11.002663	-0.048895	4.815780
234.425706	8000.516774	11.007667	-0.048889	4.815812
234.470232	8000.419295	11.012672	-0.048897	4.815784
234.349347	8000.402400	11.017677	-0.048875	4.815779
234.514705	8000.453115	11.022682	-0.048905	4.815793
234.459882	8000.514144	11.027687	-0.048895	4.815811
234.413673	8000.494188	11.032691	-0.048887	4.815806
234.481386	8000.381073	11.037696	-0.048899	4.815772
234.348220	8000.557185	11.042701	-0.048875	4.815824
234.299455	8000.459264	11.047706	-0.048866	4.815796
234.614258	8000.499588	11.052711	-0.048924	4.815806
234.529802	8000.546261	11.057715	-0.048909	4.815820
234.403685	8000.467369	11.062720	-0.048885	4.815798
234.341860	8000.537892	11.067725	-0.048874	4.815819
234.337169	8000.444954	11.072730	-0.048873	4.815792
234.310721	8000.475487	11.077735	-0.048868	4.815801
234.209088	8000.542163	11.082739	-0.048849	4.815821
234.445707	8000.457399	11.087744	-0.048893	4.815795
234.467034	8000.483368	11.092749	-0.048897	4.815802
234.310020	8000.377291	11.097754	-0.048868	4.815772
234.419365	8000.420695	11.102759	-0.048889	4.815784
234.677583	8000.460103	11.107763	-0.048937	4.815794
234.529225	8000.485461	11.112768	-0.048909	4.815803
234.212602	8000.546524	11.117773	-0.048850	4.815822
234.416550	8000.350218	11.122778	-0.048888	4.815764
234.430086	8000.476399	11.127783	-0.048891	4.815800
234.300998	8000.467911	11.132787	-0.048867	4.815798
234.460008	8000.475826	11.137792	-0.048897	4.815800
234.299386	8000.412388	11.142797	-0.048867	4.815782
234.432514	8000.561853	11.147802	-0.048892	4.815825
234.542124	8000.409920	11.152807	-0.048912	4.815780
234.472297	8000.446156	11.157811	-0.048899	4.815791
234.581256	8000.487419	11.162816	-0.048919	4.815803
234.477041	8000.528435	11.167821	-0.048900	4.815815
234.532528	8000.435403	11.172826	-0.048910	4.815788
234.542328	8000.483601	11.177831	-0.048912	4.815802
234.494874	8000.557559	11.182835	-0.048904	4.815824
234.754633	8000.463563	11.187840	-0.048952	4.815795
234.552572	8000.488051	11.192845	-0.048914	4.815803
234.427563	8000.354739	11.197850	-0.048891	4.815765
234.469507	8000.388513	11.202855	-0.048899	4.815774
234.290125	8000.467808	11.207859	-0.048866	4.815798
234.509747	8000.426534	11.212864	-0.048907	4.815785
234.211375	8000.512443	11.217869	-0.048851	4.815812
234.126519	8000.464108	11.222874	-0.048835	4.815798
234.487668	8000.489170	11.227879	-0.048903	4.815804
234.202106	8000.463206	11.232883	-0.048850	4.815798
234.306636	8000.295181	11.237888	-0.048869	4.815748
234.126380	8000.497216	11.242893	-0.048836	4.815808
234.382722	8000.473615	11.247898	-0.048883	4.815800
234.440044	8000.462805	11.252903	-0.048894	4.815796
234.516923	8000.522763	11.257907	-0.048909	4.815813
234.552591	8000.448624	11.262912	-0.048915	4.815792
234.354392	8000.522278	11.267917	-0.048878	4.815814
234.466921	8000.464327	11.272922	-0.048899	4.815797
234.595839	8000.477092	11.277927	-0.048923	4.815800
234.243052	8000.533300	11.282931	-0.048858	4.815818
234.472824	8000.481516	11.287936	-0.048901	4.815802
234.591240	8000.478100	11.292941	-0.048923	4.815800
234.621125	8000.468981	11.297946	-0.048928	4.815797
234.270004	8000.491058	11.302951	-0.048863	4.815805
234.366150	8000.525709	11.307955	-0.048881	4.815815
234.460711	8000.429040	11.312960	-0.048899	4.815786
234.503112	8000.489507	11.317965	-0.048907	4.815804
234.281478	8000.522219	11.322970	-0.048865	4.815814
234.413786	8000.479532	11.327975	-0.048890	4.815801
234.391080	8000.533609	11.332979	-0.048886	4.815817
234.512068	8000.559055	11.337984	-0.048909	4.815824
234.431705	8000.461690	11.342989	-0.048894	4.815796
234.443100	8000.466149	11.347994	-0.048896	4.815797
234.528355	8000.476073	11.352999	-0.048912	4.815800
234.743643	8000.557485	11.358003	-0.048952	4.815823
234.525710	8000.401319	11.363008	-0.048911	4.815778
234.574862	8000.464031	11.368013	-0.048921	4.815796
234.468996	8000.542381	11.373018	-0.048901	4.815819
234.526219	8000.357577	11.378023	-0.048912	4.815765
234.495550	8000.463830	11.383027	-0.048906	4.815796
234.452211	8000.462066	11.388032	-0.048898	4.815796
234.391362	8000.381029	11.393037	-0.048887	4.815773
234.456352	8000.469615	11.398042	-0.048899	4.815798
234.298422	8000.498020	11.403047	-0.048870	4.815807
234.443409	8000.552675	11.408051	-0.048897	4.815823
234.656119	8000.472862	11.413056	-0.048936	4.815798
234.633432	8000.544018	11.418061	-0.048932	4.815819
234.322474	8000.468540	11.423066	-0.048874	4.815798
234.555157	8000.482984	11.428071	-0.048918	4.815802
234.604436	8000.539294	11.433075	-0.048927	4.815818
234.643464	8000.388353	11.438080	-0.048934	4.815774
234.629414	8000.431896	11.443085	-0.048932	4.815786
234.744833	8000.468994	11.448090	-0.048953	4.815797
234.646220	8000.563473	11.453095	-0.048935	4.815825
234.625489	8000.442521	11.458099	-0.048931	4.815789
234.613546	8000.490368	11.463104	-0.048929	4.815803
234.424172	8000.565232	11.468109	-0.048894	4.815826
234.312856	8000.456691	11.473114	-0.048873	4.815795
234.509956	8000.472695	11.478119	-0.048910	4.815799
234.462067	8000.453778	11.483123	-0.048901	4.815793
234.419957	8000.490462	11.488128	-0.048893	4.815804
234.282565	8000.541616	11.493133	-0.048868	4.815820
234.498182	8000.461849	11.498138	-0.048908	4.815796
234.418738	8000.476580	11.503143	-0.048893	4.815800
234.516616	8000.510192	11.508147	-0.048911	4.815810
234.684768	8000.421118	11.513152	-0.048943	4.815783
234.806904	8000.470067	11.518157	-0.048965	4.815797
234.685219	8000.547093	11.523162	-0.048943	4.815820
234.724819	8000.352397	11.528167	-0.048950	4.815763
234.669547	8000.504152	11.533171	-0.048940	4.815807
234.525781	8000.378007	11.538176	-0.048913	4.815771
234.401387	8000.473136	11.543181	-0.048890	4.815799
234.653134	8000.572217	11.548186	-0.048937	4.815827
234.656935	8000.470876	11.553191	-0.048938	4.815798
234.415751	8000.468046	11.558195	-0.048893	4.815798
234.512633	8000.494169	11.563200	-0.048911	4.815805
234.379821	8000.471744	11.568205	-0.048886	4.815799
234.237190	8000.545229	11.573210	-0.048860	4.815821
234.532854	8000.462488	11.578215	-0.048915	4.815796
234.356114	8000.550365	11.583219	-0.048882	4.815822
234.559104	8000.395674	11.588224	-0.048920	4.815776
234.563153	8000.470465	11.593229	-0.048921	4.815798
234.641413	8000.457859	11.598234	-0.048936	4.815794
234.802635	8000.544802	11.603239	-0.048966	4.815818
234.597931	8000.448626	11.608243	-0.048928	4.815791
234.658348	8000.496576	11.613248	-0.048939	4.815805
234.661569	8000.448598	11.618253	-0.048939	4.815791
234.569000	8000.560254	11.623258	-0.048922	4.815824
234.799924	8000.463656	11.628263	-0.048965	4.815795
234.707758	8000.452562	11.633267	-0.048948	4.815792
234.619736	8000.455413	11.638272	-0.048932	4.815793
234.693899	8000.558025	11.643277	-0.048946	4.815823
234.692018	8000.448052	11.648282	-0.048946	4.815791
234.601921	8000.272608	11.653287	-0.048929	4.815740
234.526217	8000.551056	11.658291	-0.048915	4.815822
234.695679	8000.462003	11.663296	-0.048946	4.815795
234.567366	8000.553867	11.668301	-0.048923	4.815822
234.720133	8000.466678	11.673306	-0.048951	4.815796
234.751516	8000.478933	11.678311	-0.048957	4.815799
234.628978	8000.478022	11.683315	-0.048934	4.815800
234.636140	8000.486683	11.688320	-0.048936	4.815802
234.733539	8000.559783	11.693325	-0.048954	4.815823
234.667697	8000.445573	11.698330	-0.048942	4.815790
234.692890	8000.549527	11.703335	-0.048946	4.815820
234.656003	8000.388819	11.708339	-0.048939	4.815774
234.735941	8000.495794	11.713344	-0.048954	4.815804
234.804332	8000.548143	11.718349	-0.048967	4.815819
234.563555	8000.443912	11.723354	-0.048922	4.815790
234.509469	8000.481469	11.728359	-0.048912	4.815801
234.513517	8000.466596	11.733363	-0.048913	4.815797
234.614572	8000.371099	11.738368	-0.048932	4.815769
234.602319	8000.455233	11.743373	-0.048930	4.815793
234.424644	8000.563377	11.748378	-0.048897	4.815826
234.635714	8000.457918	11.753383	-0.048936	4.815794
234.625096	8000.441739	11.758387	-0.048934	4.815789
234.710575	8000.454869	11.763392	-0.048950	4.815793
234.697779	8000.514444	11.768397	-0.048948	4.815810
234.601411	8000.528901	11.773402	-0.048930	4.815815
234.702263	8000.349073	11.778407	-0.048949	4.815762
234.618118	8000.449123	11.783411	-0.048933	4.815791
234.531923	8000.558747	11.788416	-0.048917	4.815824
234.629736	8000.438646	11.793421	-0.048936	4.815788
234.651022	8000.528661	11.798426	-0.048940	4.815814
234.742347	8000.466097	11.803431	-0.048957	4.815796
234.484416	8000.547323	11.808435	-0.048909	4.815821
234.575351	8000.394021	11.813440	-0.048926	4.815775
234.646632	8000.481641	11.818445	-0.048939	4.815801
234.653106	8000.544730	11.823450	-0.048940	4.815819
234.586620	8000.464668	11.828455	-0.048928	4.815796
234.521250	8000.455076	11.833459	-0.048916	4.815793
234.747864	8000.497176	11.838464	-0.048958	4.815805
234.722036	8000.477549	11.843469	-0.048953	4.815799
234.631768	8000.448339	11.848474	-0.048937	4.815791
234.829089	8000.468616	11.853479	-0.048973	4.815796
234.835626	8000.543449	11.858483	-0.048975	4.815818
234.842338	8000.366366	11.863488	-0.048976	4.815766
234.956855	8000.376763	11.868493	-0.048997	4.815769
234.680451	8000.481175	11.873498	-0.048946	4.815800
234.660106	8000.377309	11.878503	-0.048942	4.815770
234.743198	8000.398939	11.883507	-0.048958	4.815776
234.661845	8000.502237	11.888512	-0.048943	4.815807
234.484992	8000.465222	11.893517	-0.048910	4.815797
234.662839	8000.555635	11.898522	-0.048943	4.815822
234.659057	8000.420014	11.903527	-0.048942	4.815783
234.556702	8000.535781	11.908531	-0.048923	4.815817
234.645305	8000.374968	11.913536	-0.048940	4.815769
234.650075	8000.385725	11.918541	-0.048941	4.815773
234.608737	8000.553717	11.923546	-0.048933	4.815822
234.729619	8000.482024	11.928551	-0.048956	4.815800
234.687482	8000.451458	11.933555	-0.048948	4.815792
234.783634	8000.379366	11.938560	-0.048966	4.815770
234.663708	8000.530074	11.943565	-0.048944	4.815815
234.923130	8000.435005	11.948570	-0.048992	4.815786
234.917602	8000.476551	11.953575	-0.048991	4.815798
234.719650	8000.539534	11.958579	-0.048954	4.815817
234.743473	8000.466270	11.963584	-0.048959	4.815796
234.687688	8000.472845	11.968589	-0.048948	4.815798
234.683851	8000.554981	11.973594	-0.048948	4.815822
234.672034	8000.402150	11.978599	-0.048945	4.815777
234.742620	8000.538863	11.983603	-0.048959	4.815817
234.680704	8000.463144	11.988608	-0.048947	4.815795
234.586357	8000.536343	11.993613	-0.048930	4.815817
234.722748	8000.449957	11.998618	-0.048955	4.815791
234.885815	8000.556144	12.003623	-0.048986	4.815821
234.662699	8000.525852	12.008627	-0.048944	4.815813
234.821480	8000.471851	12.013632	-0.048974	4.815797
234.946045	8000.395948	12.018637	-0.048997	4.815774
234.909418	8000.490363	12.023642	-0.048990	4.815802
234.715455	8000.476555	12.028647	-0.048954	4.815799
234.863713	8000.427721	12.033651	-0.048982	4.815784
234.739853	8000.429992	12.038656	-0.048959	4.815785
234.861271	8000.541909	12.043661	-0.048981	4.815817
234.688738	8000.535919	12.048666	-0.048949	4.815816
234.836531	8000.462527	12.053671	-0.048977	4.815794
234.667314	8000.474737	12.058675	-0.048946	4.815798
234.719771	8000.573796	12.063680	-0.048955	4.815827
235.028622	8000.383456	12.068685	-0.049013	4.815770
234.883940	8000.503877	12.073690	-0.048986	4.815806
234.862104	8000.286837	12.078695	-0.048982	4.815743
234.802465	8000.481219	12.083699	-0.048971	4.815800
234.781948	8000.404035	12.088704	-0.048967	4.815777
234.865163	8000.360554	12.093709	-0.048983	4.815764
234.687073	8000.475096	12.098714	-0.048950	4.815798
234.944373	8000.357576	12.103719	-0.048998	4.815763
234.761410	8000.472039	12.108723	-0.048964	4.815797
234.753017	8000.373703	12.113728	-0.048962	4.815769
234.706850	8000.409254	12.118733	-0.048953	4.815779
234.669051	8000.486571	12.123738	-0.048947	4.815802
234.686831	8000.485796	12.128743	-0.048950	4.815802
234.725174	8000.388216	12.133747	-0.048957	4.815773
234.707273	8000.491474	12.138752	-0.048954	4.815803
234.699971	8000.486023	12.143757	-0.048953	4.815802
234.819327	8000.558411	12.148762	-0.048975	4.815822
234.855896	8000.436251	12.153767	-0.048982	4.815786
234.876598	8000.528392	12.158771	-0.048986	4.815813
234.780345	8000.375261	12.163776	-0.048968	4.815769
234.971320	8000.554486	12.168781	-0.049003	4.815820
235.024798	8000.459286	12.173786	-0.049013	4.815792
234.749412	8000.475115	12.178791	-0.048962	4.815798
234.753007	8000.454897	12.183795	-0.048963	4.815792
234.798506	8000.475919	12.188800	-0.048971	4.815798
234.954496	8000.478449	12.193805	-0.049000	4.815798
234.788580	8000.550490	12.198810	-0.048970	4.815820
234.829179	8000.429463	12.203815	-0.048977	4.815784
234.762720	8000.431595	12.208819	-0.048965	4.815785
234.538811	8000.440786	12.213824	-0.048923	4.815789
234.562515	8000.498816	12.218829	-0.048928	4.815806
234.637014	8000.482947	12.223834	-0.048942	4.815801
234.714428	8000.502351	12.228839	-0.048956	4.815806
234.730261	8000.481263	12.233843	-0.048959	4.815800
234.560213	8000.551103	12.238848	-0.048928	4.815821
234.616404	8000.466621	12.243853	-0.048938	4.815796
234.595804	8000.390505	12.248858	-0.048934	4.815774
234.751772	8000.384494	12.253863	-0.048963	4.815772
234.740394	8000.502801	12.258867	-0.048961	4.815806
234.663003	8000.275256	12.263872	-0.048947	4.815740
234.811161	8000.434572	12.268877	-0.048975	4.815786
234.894066	8000.509572	12.273882	-0.048990	4.815808
234.917877	8000.394678	12.278887	-0.048995	4.815774
234.645994	8000.457532	12.283891	-0.048944	4.815793
234.789638	8000.484413	12.288896	-0.048971	4.815801
234.862134	8000.389521	12.293901	-0.048984	4.815773
234.717201	8000.476846	12.298906	-0.048957	4.815799
234.724677	8000.388374	12.303911	-0.048959	4.815773
235.034597	8000.484127	12.308915	-0.049017	4.815799
234.934489	8000.369362	12.313920	-0.048998	4.815766
234.757948	8000.385724	12.318925	-0.048965	4.815772
234.784556	8000.482230	12.323930	-0.048970	4.815800
234.940329	8000.486890	12.328935	-0.048999	4.815801
234.658446	8000.547448	12.333939	-0.048947	4.815820
234.900661	8000.451032	12.338944	-0.048992	4.815790
235.060539	8000.480311	12.343949	-0.049022	4.815798
234.910441	8000.471482	12.348954	-0.048994	4.815796
234.812569	8000.481645	12.353959	-0.048976	4.815800
234.723913	8000.395887	12.358963	-0.048959	4.815775
234.903091	8000.450029	12.363968	-0.048993	4.815790
234.866647	8000.462253	12.368973	-0.048986	4.815794
234.819904	8000.542628	12.373978	-0.048977	4.815818
234.861666	8000.283919	12.378983	-0.048985	4.815742
234.740050	8000.536008	12.383987	-0.048963	4.815816
234.918935	8000.479130	12.388992	-0.048996	4.815798
234.904885	8000.485313	12.393997	-0.048993	4.815800
234.670475	8000.538099	12.399002	-0.048950	4.815817
234.758106	8000.393281	12.404007	-0.048966	4.815774
235.034579	8000.463942	12.409011	-0.049018	4.815793
235.085291	8000.470105	12.414016	-0.049027	4.815795
234.974579	8000.533433	12.419021	-0.049007	4.815814
235.095117	8000.447857	12.424026	-0.049029	4.815789
235.116889	8000.473834	12.429031	-0.049033	4.815796
234.954906	8000.552343	12.434035	-0.049003	4.815820
234.808681	8000.454978	12.439040	-0.048976	4.815792
235.045963	8000.375562	12.444045	-0.049020	4.815768
235.042082	8000.470507	12.449050	-0.049020	4.815795
234.994264	8000.476143	12.454055	-0.049011	4.815797
235.048658	8000.433263	12.459059	-0.049021	4.815784
235.104516	8000.406418	12.464064	-0.049031	4.815776
235.181464	8000.559247	12.469069	-0.049046	4.815821
235.136284	8000.462449	12.474074	-0.049037	4.815793
235.026791	8000.469222	12.479079	-0.049017	4.815795
234.945797	8000.477523	12.484083	-0.049002	4.815798
234.994881	8000.454838	12.489088	-0.049011	4.815791
234.888394	8000.471266	12.494093	-0.048992	4.815796
234.769733	8000.552612	12.499098	-0.048970	4.815821
234.778795	8000.392646	12.504103	-0.048971	4.815774
234.793274	8000.481483	12.509107	-0.048974	4.815800
234.868895	8000.466700	12.514112	-0.048988	4.815795
234.818072	8000.477624	12.519117	-0.048979	4.815798
234.686077	8000.476561	12.524122	-0.048954	4.815799
235.046593	8000.450376	12.529127	-0.049021	4.815789
234.897580	8000.490668	12.534131	-0.048994	4.815802
234.636539	8000.450155	12.539136	-0.048945	4.815791
234.789386	8000.549771	12.544141	-0.048974	4.815820
234.980333	8000.467470	12.549146	-0.049009	4.815795
234.861106	8000.485827	12.554151	-0.048987	4.815801
234.743324	8000.473251	12.559155	-0.048965	4.815798
234.825286	8000.466043	12.564160	-0.048981	4.815795
234.896948	8000.467208	12.569165	-0.048994	4.815795
235.125099	8000.474107	12.574170	-0.049037	4.815796
235.142646	8000.464789	12.579175	-0.049040	4.815793
235.121044	8000.465512	12.584179	-0.049036	4.815793
235.064839	8000.479551	12.589184	-0.049025	4.815798
235.009387	8000.406072	12.594189	-0.049015	4.815777
235.164378	8000.476902	12.599194	-0.049044	4.815797
235.071280	8000.417758	12.604199	-0.049027	4.815780
235.089797	8000.438344	12.609203	-0.049030	4.815786
235.201158	8000.451893	12.614208	-0.049051	4.815789
235.212112	8000.462750	12.619213	-0.049053	4.815792
235.012603	8000.484077	12.624218	-0.049016	4.815799
235.207659	8000.350605	12.629223	-0.049052	4.815759
234.968934	8000.423603	12.634227	-0.049008	4.815782
234.923931	8000.441026	12.639232	-0.049000	4.815787
234.923032	8000.477310	12.644237	-0.049000	4.815798
234.956439	8000.457574	12.649242	-0.049006	4.815792
234.971041	8000.496243	12.654247	-0.049009	4.815803
234.901914	8000.459903	12.659251	-0.048996	4.815793
234.930111	8000.371766	12.664256	-0.049001	4.815767
234.854263	8000.481558	12.669261	-0.048987	4.815799
234.807969	8000.463735	12.674266	-0.048979	4.815794
234.971215	8000.384188	12.679271	-0.049009	4.815770
234.947619	8000.550334	12.684275	-0.049005	4.815819
234.935009	8000.474345	12.689280	-0.049002	4.815797
235.131929	8000.332364	12.694285	-0.049039	4.815754
235.086877	8000.475745	12.699290	-0.049031	4.815797
235.016784	8000.378545	12.704295	-0.049018	4.815769
235.042890	8000.371500	12.709299	-0.049023	4.815766
235.147052	8000.428698	12.714304	-0.049042	4.815783
234.905445	8000.486705	12.719309	-0.048997	4.815801
234.941498	8000.459540	12.724314	-0.049004	4.815793
235.145641	8000.394532	12.729319	-0.049042	4.815773
235.337492	8000.488376	12.734323	-0.049078	4.815799
235.152948	8000.448032	12.739328	-0.049044	4.815788
235.067388	8000.421033	12.744333	-0.049028	4.815781
235.049940	8000.402609	12.749338	-0.049024	4.815775
235.297679	8000.359656	12.754343	-0.049071	4.815762
235.027372	8000.466301	12.759347	-0.049020	4.815794
235.035009	8000.473902	12.764352	-0.049022	4.815796
235.098643	8000.373528	12.769357	-0.049034	4.815767
235.080526	8000.486390	12.774362	-0.049030	4.815800
235.122589	8000.500953	12.779367	-0.049038	4.815804
234.938705	8000.452081	12.784371	-0.049004	4.815790
234.796754	8000.383607	12.789376	-0.048978	4.815771
235.114684	8000.248921	12.794381	-0.049037	4.815730
234.837769	8000.484620	12.799386	-0.048986	4.815800
234.792368	8000.383550	12.804391	-0.048977	4.815771
234.798887	8000.523496	12.809395	-0.048978	4.815812
234.919695	8000.465679	12.814400	-0.049001	4.815794
235.098865	8000.469651	12.819405	-0.049034	4.815795
234.875271	8000.553569	12.824410	-0.048993	4.815820
235.137009	8000.470278	12.829415	-0.049042	4.815795
235.087040	8000.529252	12.834419	-0.049032	4.815812
235.045348	8000.468805	12.839424	-0.049025	4.815795
235.142463	8000.473584	12.844429	-0.049043	4.815796
235.205735	8000.551470	12.849434	-0.049055	4.815818
235.336830	8000.473537	12.854439	-0.049079	4.815795
235.208898	8000.381805	12.859443	-0.049055	4.815769
235.253967	8000.525579	12.864448	-0.049064	4.815810
235.266966	8000.348596	12.869453	-0.049066	4.815759
234.992580	8000.467985	12.874458	-0.049015	4.815795
234.924984	8000.480772	12.879463	-0.049003	4.815799
234.980546	8000.478474	12.884467	-0.049013	4.815798
234.920678	8000.439082	12.889472	-0.049002	4.815787
235.066709	8000.345379	12.894477	-0.049029	4.815759
235.088130	8000.531468	12.899482	-0.049033	4.815813
235.191681	8000.411459	12.904487	-0.049053	4.815777
234.992273	8000.471216	12.909491	-0.049016	4.815796
234.952943	8000.469517	12.914496	-0.049008	4.815795
235.180848	8000.502032	12.919501	-0.049051	4.815804
234.892801	8000.467486	12.924506	-0.048997	4.815795
235.153065	8000.483445	12.929511	-0.049046	4.815798
235.063520	8000.472393	12.934515	-0.049029	4.815796
235.133670	8000.374260	12.939520	-0.049042	4.815767
234.997782	8000.496958	12.944525	-0.049017	4.815803
234.951285	8000.462052	12.949530	-0.049008	4.815793
235.031424	8000.421723	12.954535	-0.049023	4.815781
235.036955	8000.469853	12.959539	-0.049024	4.815795
234.852419	8000.502097	12.964544	-0.048990	4.815805
235.088530	8000.495249	12.969549	-0.049034	4.815802
235.144770	8000.508974	12.974554	-0.049045	4.815806
235.157837	8000.454750	12.979559	-0.049047	4.815790
235.179139	8000.562913	12.984563	-0.049051	4.815822
235.198336	8000.471427	12.989568	-0.049055	4.815795
235.144170	8000.396900	12.994573	-0.049045	4.815773
235.182223	8000.554438	12.999578	-0.049052	4.815819
235.150451	8000.331897	13.004583	-0.049046	4.815754
235.015728	8000.451411	13.009587	-0.049021	4.815790
235.300181	8000.547822	13.014592	-0.049074	4.815817
235.406983	8000.404381	13.019597	-0.049094	4.815774
235.018510	8000.536867	13.024602	-0.049022	4.815815
235.237162	8000.465689	13.029607	-0.049062	4.815793
235.245484	8000.442345	13.034611	-0.049064	4.815786
235.006123	8000.480106	13.039616	-0.049020	4.815798
235.062871	8000.468220	13.044621	-0.049030	4.815794
235.171053	8000.552170	13.049626	-0.049050	4.815818
235.039445	8000.387792	13.054631	-0.049026	4.815771
235.104080	8000.465699	13.059635	-0.049038	4.815793
234.983618	8000.477631	13.064640	-0.049016	4.815798
235.203730	8000.475862	13.069645	-0.049057	4.815796
235.060447	8000.473547	13.074650	-0.049030	4.815796
235.088248	8000.393943	13.079655	-0.049035	4.815773
235.167759	8000.503048	13.084659	-0.049050	4.815804
235.250442	8000.469165	13.089664	-0.049066	4.815794
235.305867	8000.581083	13.094669	-0.049076	4.815826
235.242720	8000.467982	13.099674	-0.049064	4.815793
235.086170	8000.461183	13.104679	-0.049035	4.815792
235.037735	8000.456134	13.109683	-0.049026	4.815791
234.961658	8000.481594	13.114688	-0.049012	4.815799
235.115585	8000.369873	13.119693	-0.049041	4.815765
235.018761	8000.477191	13.124698	-0.049023	4.815797
235.228908	8000.448574	13.129703	-0.049062	4.815788
235.136528	8000.363822	13.134707	-0.049045	4.815764
235.198214	8000.475840	13.139712	-0.049056	4.815796
235.191225	8000.373256	13.144717	-0.049055	4.815766
235.034567	8000.352579	13.149722	-0.049026	4.815761
235.168109	8000.204235	13.154727	-0.049051	4.815717
235.091132	8000.501881	13.159731	-0.049037	4.815804
235.008846	8000.377797	13.164736	-0.049021	4.815768
235.157318	8000.492287	13.169741	-0.049049	4.815801
235.247955	8000.543930	13.174746	-0.049066	4.815816
235.173476	8000.464804	13.179751	-0.049052	4.815793
235.198028	8000.385147	13.184755	-0.049057	4.815769
235.172718	8000.554468	13.189760	-0.049052	4.815819
235.113923	8000.395538	13.194765	-0.049041	4.815773
235.181746	8000.505521	13.199770	-0.049054	4.815805
235.407360	8000.451535	13.204775	-0.049096	4.815788
235.191735	8000.294337	13.209779	-0.049056	4.815743
235.286575	8000.447455	13.214784	-0.049074	4.815787
235.377229	8000.374205	13.219789	-0.049091	4.815765
235.220010	8000.364193	13.224794	-0.049061	4.815763
235.153339	8000.479471	13.229799	-0.049049	4.815797
235.302191	8000.440255	13.234803	-0.049077	4.815785
235.310233	8000.429715	13.239808	-0.049078	4.815782
235.145877	8000.475095	13.244813	-0.049048	4.815796
235.224815	8000.560708	13.249818	-0.049063	4.815821
235.450308	8000.391434	13.254823	-0.049105	4.815770
235.395125	8000.480212	13.259827	-0.049094	4.815796
235.205639	8000.489959	13.264832	-0.049059	4.815800
235.211662	8000.397193	13.269837	-0.049060	4.815773
235.100846	8000.557658	13.274842	-0.049040	4.815820
235.149117	8000.370571	13.279847	-0.049049	4.815765
235.183842	8000.483221	13.284851	-0.049055	4.815798
235.108653	8000.464930	13.289856	-0.049041	4.815793
235.366823	8000.158484	13.294861	-0.049089	4.815702
235.157886	8000.486018	13.299866	-0.049051	4.815799
235.258607	8000.388379	13.304871	-0.049069	4.815770
235.166828	8000.476565	13.309875	-0.049053	4.815796
235.248262	8000.477888	13.314880	-0.049068	4.815796
235.288262	8000.288533	13.319885	-0.049075	4.815741
235.187344	8000.495059	13.324890	-0.049057	4.815802
235.093787	8000.477537	13.329895	-0.049039	4.815797
235.108033	8000.460693	13.334899	-0.049042	4.815792
235.159988	8000.493563	13.339904	-0.049052	4.815801
235.269306	8000.409941	13.344909	-0.049072	4.815776
235.155124	8000.461470	13.349914	-0.049051	4.815792
235.195938	8000.473878	13.354919	-0.049058	4.815795
235.414014	8000.350385	13.359923	-0.049099	4.815758
235.285652	8000.456125	13.364928	-0.049075	4.815790
235.340234	8000.404708	13.369933	-0.049085	4.815774
235.154097	8000.475355	13.374938	-0.049051	4.815796
235.319963	8000.478045	13.379943	-0.049082	4.815796
235.070022	8000.477206	13.384947	-0.049035	4.815797
235.205223	8000.468725	13.389952	-0.049061	4.815794
235.221811	8000.388939	13.394957	-0.049064	4.815770
235.190423	8000.431134	13.399962	-0.049058	4.815783
235.314415	8000.421404	13.404967	-0.049081	4.815779
235.435639	8000.469272	13.409971	-0.049104	4.815793
235.126758	8000.458939	13.414976	-0.049046	4.815791
235.247109	8000.389373	13.419981	-0.049069	4.815770
235.178390	8000.475797	13.424986	-0.049056	4.815796
235.231033	8000.476654	13.429991	-0.049066	4.815796
235.007038	8000.458089	13.434995	-0.049024	4.815792
235.250425	8000.550632	13.440000	-0.049070	4.815818
235.309616	8000.387206	13.445005	-0.049081	4.815769
235.035836	8000.460704	13.450010	-0.049030	4.815792
235.260077	8000.477148	13.455015	-0.049071	4.815796
235.334736	8000.378020	13.460019	-0.049085	4.815767
235.140340	8000.480557	13.465024	-0.049049	4.815798
235.024421	8000.399694	13.470029	-0.049028	4.815774
235.248075	8000.546358	13.475034	-0.049070	4.815816
235.229346	8000.459596	13.480039	-0.049066	4.815791
235.349461	8000.464747	13.485043	-0.049088	4.815792
235.521745	8000.445124	13.490048	-0.049121	4.815785
235.547275	8000.378292	13.495053	-0.049125	4.815766
235.369390	8000.456545	13.500058	-0.049092	4.815789
235.311861	8000.474833	13.505063	-0.049082	4.815795
235.286804	8000.481904	13.510067	-0.049077	4.815797
235.089302	8000.551299	13.515072	-0.049040	4.815818
235.298329	8000.483168	13.520077	-0.049079	4.815798
235.154432	8000.446685	13.525082	-0.049053	4.815788
235.183307	8000.389514	13.530087	-0.049058	4.815771
235.237492	8000.413880	13.535091	-0.049068	4.815778
235.217066	8000.475467	13.540096	-0.049064	4.815796
235.294753	8000.394535	13.545101	-0.049079	4.815772
235.193400	8000.485768	13.550106	-0.049060	4.815799
235.296742	8000.477839	13.555111	-0.049079	4.815796
235.250066	8000.471751	13.560115	-0.049071	4.815794
235.160542	8000.461767	13.565120	-0.049054	4.815792
235.209989	8000.380378	13.570125	-0.049063	4.815768
235.155484	8000.477707	13.575130	-0.049053	4.815797
235.309214	8000.497279	13.580135	-0.049082	4.815802
235.308819	8000.374520	13.585139	-0.049082	4.815766
235.272622	8000.495629	13.590144	-0.049075	4.815801
235.294215	8000.490646	13.595149	-0.049079	4.815800
235.134762	8000.542511	13.600154	-0.049050	4.815816
235.166338	8000.417067	13.605159	-0.049056	4.815779
235.160439	8000.474619	13.610163	-0.049055	4.815796
235.091032	8000.555695	13.615168	-0.049042	4.815820
235.345352	8000.316435	13.620173	-0.049089	4.815749
235.323953	8000.498629	13.625178	-0.049085	4.815802
235.407197	8000.207498	13.630183	-0.049101	4.815716
235.322666	8000.312880	13.635187	-0.049085	4.815748
235.137863	8000.504171	13.640192	-0.049051	4.815804
235.322725	8000.476212	13.645197	-0.049085	4.815795
235.120709	8000.547669	13.650202	-0.049048	4.815817
235.245181	8000.558229	13.655207	-0.049071	4.815820
235.392578	8000.470953	13.660211	-0.049098	4.815793
235.298399	8000.458758	13.665216	-0.049081	4.815790
235.367636	8000.404376	13.670221	-0.049094	4.815774
235.254487	8000.475137	13.675226	-0.049073	4.815795
235.288029	8000.476752	13.680231	-0.049079	4.815796
235.500522	8000.443903	13.685235	-0.049119	4.815785
235.337057	8000.474353	13.690240	-0.049088	4.815795
235.482979	8000.359299	13.695245	-0.049116	4.815760
235.145709	8000.436039	13.700250	-0.049053	4.815784
235.125776	8000.461341	13.705255	-0.049049	4.815792
235.223451	8000.462926	13.710259	-0.049068	4.815792
235.110347	8000.371434	13.715264	-0.049046	4.815766
235.346428	8000.403014	13.720269	-0.049090	4.815774
235.308458	8000.544377	13.725274	-0.049084	4.815815
235.366755	8000.434309	13.730279	-0.049094	4.815783
235.402412	8000.475455	13.735283	-0.049101	4.815795
235.215193	8000.451080	13.740288	-0.049066	4.815789
235.526916	8000.450793	13.745293	-0.049124	4.815787
235.360535	8000.475859	13.750298	-0.049093	4.815795
235.357378	8000.378674	13.755303	-0.049093	4.815767
235.167912	8000.554945	13.760307	-0.049058	4.815819
235.249318	8000.444184	13.765312	-0.049073	4.815786
235.318257	8000.497611	13.770317	-0.049086	4.815802
235.131274	8000.533017	13.775322	-0.049051	4.815813
235.433116	8000.376721	13.780327	-0.049107	4.815766
235.319642	8000.488041	13.785331	-0.049086	4.815799
235.309693	8000.460130	13.790336	-0.049084	4.815791
235.373369	8000.489987	13.795341	-0.049096	4.815799
235.284613	8000.492825	13.800346	-0.049080	4.815800
235.236462	8000.481376	13.805351	-0.049071	4.815797
235.447765	8000.406877	13.810355	-0.049110	4.815774
235.352094	8000.544103	13.815360	-0.049093	4.815815
235.521627	8000.434769	13.820365	-0.049124	4.815782
235.316029	8000.504033	13.825370	-0.049086	4.815803
235.452944	8000.402710	13.830375	-0.049112	4.815773
235.476104	8000.398820	13.835379	-0.049116	4.815772
235.331378	8000.554467	13.840384	-0.049089	4.815818
235.551908	8000.373370	13.845389	-0.049130	4.815764
235.483295	8000.482213	13.850394	-0.049117	4.815796
235.489427	8000.433214	13.855399	-0.049119	4.815782
235.214696	8000.411693	13.860403	-0.049068	4.815777
235.392396	8000.476486	13.865408	-0.049101	4.815795
235.479479	8000.166204	13.870413	-0.049117	4.815704
235.455611	8000.499936	13.875418	-0.049113	4.815802
235.344928	8000.487475	13.880423	-0.049092	4.815798
235.320043	8000.370724	13.885427	-0.049087	4.815764
235.147196	8000.551534	13.890432	-0.049055	4.815818
235.361731	8000.369273	13.895437	-0.049095	4.815764
235.443873	8000.467747	13.900442	-0.049111	4.815792
235.371407	8000.486860	13.905447	-0.049097	4.815798
235.341807	8000.429810	13.910451	-0.049092	4.815782
235.391045	8000.460501	13.915456	-0.049101	4.815790
235.395176	8000.481922	13.920461	-0.049102	4.815797
235.414647	8000.461961	13.925466	-0.049106	4.815791
235.357210	8000.363897	13.930471	-0.049095	4.815762
235.569790	8000.478359	13.935475	-0.049135	4.815795
235.409274	8000.564365	13.940480	-0.049105	4.815821
235.392068	8000.469087	13.945485	-0.049102	4.815793
235.549768	8000.372370	13.950490	-0.049131	4.815764
235.332543	8000.440379	13.955495	-0.049091	4.815785
235.327579	8000.417887	13.960499	-0.049090	4.815778
235.186987	8000.470056	13.965504	-0.049064	4.815794
235.374488	8000.436803	13.970509	-0.049099	4.815784
235.439205	8000.453867	13.975514	-0.049111	4.815788
235.369487	8000.474093	13.980519	-0.049098	4.815794
235.478075	8000.479058	13.985523	-0.049118	4.815795
235.400450	8000.557866	13.990528	-0.049104	4.815819
235.401454	8000.402037	13.995533	-0.049104	4.815773
235.395578	8000.468130	14.000538	-0.049103	4.815793
235.268960	8000.487434	14.005543	-0.049079	4.815799
235.357582	8000.388532	14.010547	-0.049096	4.815769
235.216505	8000.549575	14.015552	-0.049070	4.815817
235.402793	8000.481075	14.020557	-0.049104	4.815796
235.225293	8000.486747	14.025562	-0.049071	4.815799
235.248828	8000.435894	14.030567	-0.049076	4.815784
235.378132	8000.562886	14.035571	-0.049100	4.815820
235.393204	8000.474535	14.040576	-0.049103	4.815794
235.403940	8000.405328	14.045581	-0.049105	4.815774
235.268521	8000.551519	14.050586	-0.049080	4.815818
235.441171	8000.442235	14.055591	-0.049112	4.815785
235.323094	8000.476622	14.060595	-0.049090	4.815795
235.526795	8000.447900	14.065600	-0.049128	4.815786
235.556543	8000.478276	14.070605	-0.049134	4.815795
235.390608	8000.555654	14.075610	-0.049103	4.815818
235.456327	8000.480933	14.080615	-0.049115	4.815796
235.534987	8000.466199	14.085619	-0.049130	4.815791
235.518688	8000.568417	14.090624	-0.049127	4.815821
235.503241	8000.389905	14.095629	-0.049124	4.815769
235.383843	8000.464835	14.100634	-0.049102	4.815792
235.419256	8000.485695	14.105639	-0.049108	4.815798
235.529046	8000.379663	14.110643	-0.049129	4.815766
235.455630	8000.468146	14.115648	-0.049115	4.815792
235.554893	8000.480433	14.120653	-0.049134	4.815795
235.531150	8000.471513	14.125658	-0.049129	4.815793
235.458034	8000.459660	14.130663	-0.049116	4.815790
235.605613	8000.245359	14.135667	-0.049143	4.815726
235.409571	8000.473830	14.140672	-0.049107	4.815794
235.482273	8000.394952	14.145677	-0.049121	4.815771
235.524110	8000.549349	14.150682	-0.049128	4.815816
235.585255	8000.486296	14.155687	-0.049140	4.815797
235.537804	8000.454576	14.160691	-0.049131	4.815788
235.567480	8000.482815	14.165696	-0.049137	4.815796
235.769954	8000.415645	14.170701	-0.049174	4.815775
235.487537	8000.456979	14.175706	-0.049122	4.815789
235.340687	8000.470619	14.180711	-0.049095	4.815793
235.575590	8000.487236	14.185715	-0.049138	4.815797
235.366747	8000.450768	14.190720	-0.049100	4.815788
235.377808	8000.341004	14.195725	-0.049102	4.815755
235.289446	8000.500765	14.200730	-0.049085	4.815803
235.630654	8000.392074	14.205735	-0.049149	4.815769
235.606320	8000.350054	14.210739	-0.049144	4.815757
235.579856	8000.347496	14.215744	-0.049139	4.815756
235.543633	8000.401355	14.220749	-0.049133	4.815772
235.400526	8000.453484	14.225754	-0.049106	4.815788
235.499144	8000.298168	14.230759	-0.049125	4.815742
235.491431	8000.492327	14.235763	-0.049123	4.815799
235.580196	8000.457475	14.240768	-0.049140	4.815789
235.444476	8000.390167	14.245773	-0.049115	4.815769
235.303664	8000.557620	14.250778	-0.049089	4.815819
235.593598	8000.375511	14.255783	-0.049142	4.815764
235.446034	8000.488414	14.260787	-0.049115	4.815798
235.353258	8000.412194	14.265792	-0.049098	4.815776
235.471781	7999.524944	14.270797	-0.049119	4.815516

235.431520	7996.241289	14.275802	-0.049110	4.814556
235.244222	7990.663179	14.280807	-0.049071	4.812925
235.340517	7983.948289	14.285811	-0.049085	4.810959
235.327749	7976.611911	14.290816	-0.049078	4.808811
235.322066	7969.047734	14.295821	-0.049072	4.806595
235.353563	7961.235237	14.300826	-0.049073	4.804305
235.427017	7953.344070	14.305831	-0.049081	4.801990
235.508929	7945.416386	14.310835	-0.049092	4.799664
235.376454	7937.430894	14.315840	-0.049062	4.797321
235.234893	7929.429037	14.320845	-0.049030	4.794971
235.247501	7921.384499	14.325850	-0.049027	4.792608
234.993529	7913.373095	14.330855	-0.048975	4.790254
235.152153	7905.429834	14.335859	-0.048999	4.787917
234.869370	7897.394191	14.340864	-0.048941	4.785553
234.749536	7889.449651	14.345869	-0.048914	4.783215
234.830314	7881.426944	14.350874	-0.048924	4.780852
234.847817	7873.428535	14.355879	-0.048922	4.778495
234.708112	7865.427810	14.360883	-0.048891	4.776136
234.536142	7857.393654	14.365888	-0.048854	4.773767
234.626411	7849.361558	14.370893	-0.048865	4.771396
234.626063	7841.395735	14.375898	-0.048860	4.769044
234.593354	7833.394365	14.380903	-0.048849	4.766680
234.546140	7825.390476	14.385907	-0.048835	4.764315
234.431028	7817.391901	14.390912	-0.048808	4.761950
234.589650	7809.374144	14.395917	-0.048833	4.759577
234.329178	7801.446248	14.400922	-0.048779	4.757231
234.377660	7793.331907	14.405927	-0.048783	4.754828
234.243759	7785.334472	14.410931	-0.048753	4.752459
234.359837	7777.263766	14.415936	-0.048769	4.750066
234.317770	7769.331163	14.420941	-0.048756	4.747713
234.095589	7761.316501	14.425946	-0.048710	4.745335
233.910315	7753.333659	14.430951	-0.048670	4.742966
234.152425	7745.347606	14.435955	-0.048710	4.740593
234.015990	7737.348099	14.440960	-0.048679	4.738215
233.780472	7729.379005	14.445965	-0.048630	4.735846
233.777637	7721.315474	14.450970	-0.048625	4.733448
233.986954	7713.267438	14.455975	-0.048658	4.731051
234.035856	7705.302659	14.460979	-0.048662	4.728679
233.774877	7697.309792	14.465984	-0.048609	4.726298
233.681752	7689.346595	14.470989	-0.048586	4.723925
233.712233	7681.352910	14.475994	-0.048587	4.721541
233.572900	7673.283410	14.480999	-0.048556	4.719133
233.679931	7665.349711	14.486003	-0.048570	4.716764
233.568114	7657.292854	14.491008	-0.048544	4.714357
233.477800	7649.305076	14.496013	-0.048522	4.711970
233.208335	7641.274120	14.501018	-0.048467	4.709570
233.268269	7633.338454	14.506023	-0.048473	4.707195
233.242573	7625.249757	14.511027	-0.048463	4.704774
232.895576	7617.319352	14.516032	-0.048393	4.702400
233.108448	7609.318729	14.521037	-0.048428	4.700002
233.045079	7601.349465	14.526042	-0.048411	4.697613
232.799913	7593.299888	14.531047	-0.048360	4.695199
232.890679	7585.350222	14.536051	-0.048372	4.692813
233.015812	7577.237410	14.541056	-0.048390	4.690377
232.885478	7569.298740	14.546061	-0.048361	4.687993
232.714677	7561.290212	14.551066	-0.048324	4.685586
232.814072	7553.315344	14.556071	-0.048337	4.683188
232.964590	7545.300189	14.561075	-0.048360	4.680776
232.668465	7537.326294	14.566080	-0.048300	4.678376
232.635204	7529.332998	14.571085	-0.048288	4.675969
232.854037	7521.238310	14.576090	-0.048324	4.673529
232.669470	7513.135648	14.581095	-0.048284	4.671086
232.565019	7505.249755	14.586099	-0.048260	4.668708
232.315638	7497.214291	14.591104	-0.048208	4.666283
232.373113	7489.232858	14.596109	-0.048214	4.663873
232.217797	7481.260967	14.601114	-0.048179	4.661464
232.317414	7473.230117	14.606119	-0.048193	4.659037
232.396735	7465.286952	14.611123	-0.048202	4.656634
232.311395	7457.232868	14.616128	-0.048181	4.654197
232.064010	7449.225884	14.621133	-0.048130	4.651773
232.048229	7441.201122	14.626138	-0.048122	4.649343
232.007926	7433.183600	14.631143	-0.048109	4.646913
232.045532	7425.212674	14.636147	-0.048111	4.644496
232.094088	7417.241798	14.641152	-0.048115	4.642077
232.058147	7409.243032	14.646157	-0.048103	4.639649
231.755205	7401.263442	14.651162	-0.048042	4.637226
231.845276	7393.205534	14.656167	-0.048053	4.634778
231.921909	7385.214463	14.661171	-0.048062	4.632348
231.901500	7377.126902	14.666176	-0.048053	4.629888
231.704813	7369.231167	14.671181	-0.048012	4.627485
231.588471	7361.157227	14.676186	-0.047985	4.625026
231.651139	7353.166608	14.681191	-0.047991	4.622592
231.582061	7345.219049	14.686195	-0.047973	4.620169
231.410446	7337.218371	14.691200	-0.047936	4.617729
231.552786	7329.227091	14.696205	-0.047958	4.615290
231.444361	7321.211430	14.701210	-0.047932	4.612843
231.279199	7313.111208	14.706215	-0.047896	4.610369
231.425099	7305.210251	14.711219	-0.047918	4.607954
231.295350	7297.149297	14.716224	-0.047889	4.605489
231.361504	7289.217985	14.721229	-0.047896	4.603062
231.285557	7281.197215	14.726234	-0.047877	4.600606
231.076033	7273.189106	14.731239	-0.047833	4.598153
231.013703	7265.185122	14.736243	-0.047816	4.595700
230.905794	7257.096970	14.741248	-0.047791	4.593220
230.971204	7249.101399	14.746253	-0.047798	4.590767
230.791398	7241.127908	14.751258	-0.047759	4.588320
230.722935	7233.087346	14.756263	-0.047741	4.585850
230.703019	7225.165800	14.761267	-0.047732	4.583416
230.868749	7217.115991	14.766272	-0.047758	4.580941
230.602727	7209.141766	14.771277	-0.047703	4.578488
230.649513	7201.130375	14.776282	-0.047707	4.576022
230.619670	7193.096185	14.781287	-0.047696	4.573548
230.558988	7185.115094	14.786291	-0.047680	4.571089
230.394889	7177.100245	14.791296	-0.047644	4.568618
230.641071	7169.171163	14.796301	-0.047685	4.566172
230.588031	7161.125106	14.801306	-0.047670	4.563689
230.365697	7153.169094	14.806311	-0.047623	4.561232
230.448387	7145.214066	14.811315	-0.047633	4.558774
230.491442	7137.175648	14.816320	-0.047636	4.556289
230.370512	7129.184794	14.821325	-0.047609	4.553818
230.198915	7121.096727	14.826330	-0.047571	4.551315
230.297510	7113.051067	14.831335	-0.047585	4.548824
230.273142	7105.099116	14.836339	-0.047575	4.546360
230.026673	7097.107443	14.841344	-0.047524	4.543882
230.076255	7089.135602	14.846349	-0.047528	4.541410
230.094617	7081.161241	14.851354	-0.047526	4.538936
230.006316	7073.144649	14.856359	-0.047505	4.536446
229.843169	7065.157096	14.861363	-0.047469	4.533965
229.762572	7057.080054	14.866368	-0.047449	4.531454
229.560854	7049.124773	14.871373	-0.047406	4.528979
229.684783	7041.116468	14.876378	-0.047424	4.526488
229.751801	7033.117957	14.881383	-0.047431	4.523998
229.684456	7025.176929	14.886387	-0.047414	4.521524
229.482475	7017.102116	14.891392	-0.047371	4.519007
229.616891	7009.181387	14.896397	-0.047391	4.516537
229.620453	7001.093946	14.901402	-0.047386	4.514013
229.409176	6992.972809	14.906407	-0.047342	4.511477
229.522157	6985.053436	14.911411	-0.047358	4.509004
229.277170	6977.027606	14.916416	-0.047307	4.506494
229.324024	6969.071655	14.921421	-0.047310	4.504007
229.213770	6961.114516	14.926426	-0.047285	4.501516
229.099770	6953.075134	14.931431	-0.047258	4.498999
229.028331	6945.113637	14.936435	-0.047240	4.496505
229.065386	6937.038052	14.941440	-0.047242	4.493974
229.134137	6929.053286	14.946445	-0.047249	4.491470
229.003429	6921.057034	14.951450	-0.047220	4.488961
228.706397	6913.005362	14.956455	-0.047159	4.486432
228.884128	6905.059762	14.961459	-0.047187	4.483936
228.895929	6897.058703	14.966464	-0.047184	4.481422
228.691252	6889.080338	14.971469	-0.047141	4.478912
228.823511	6881.109800	14.976474	-0.047161	4.476404
228.743948	6873.014190	14.981479	-0.047140	4.473855
228.896356	6865.035541	14.986483	-0.047164	4.471342
228.636903	6856.980901	14.991488	-0.047110	4.468803
228.708117	6849.026051	14.996493	-0.047118	4.466294
228.792136	6841.028021	15.001498	-0.047129	4.463771
228.519619	6833.068449	15.006503	-0.047073	4.461256
228.479309	6825.030607	15.011507	-0.047060	4.458717
228.392592	6817.040404	15.016512	-0.047039	4.456191
228.505818	6809.013757	15.021517	-0.047055	4.453653
228.454121	6801.033219	15.026522	-0.047040	4.451127
228.411567	6793.007835	15.031527	-0.047027	4.448586
228.130607	6785.027652	15.036531	-0.046970	4.446056
228.188877	6776.998345	15.041536	-0.046975	4.443511
228.291439	6769.046821	15.046541	-0.046989	4.440990
228.283327	6761.031485	15.051546	-0.046983	4.438446
227.977994	6753.038679	15.056551	-0.046921	4.435906
227.945249	6745.010362	15.061555	-0.046909	4.433355
227.804320	6736.977446	15.066560	-0.046878	4.430801
227.815256	6728.953878	15.071565	-0.046875	4.428249
227.664729	6720.991260	15.076570	-0.046842	4.425714
227.575919	6712.985306	15.081575	-0.046820	4.423164
227.685777	6704.992751	15.086579	-0.046835	4.420617
227.439994	6696.984779	15.091584	-0.046784	4.418063
227.386638	6689.021596	15.096589	-0.046769	4.415522
227.429470	6680.979378	15.101594	-0.046772	4.412955
227.490266	6672.924931	15.106599	-0.046778	4.410383
227.375777	6664.995192	15.111603	-0.046752	4.407848
227.221664	6656.934066	15.116608	-0.046718	4.405270
227.320410	6648.979877	15.121613	-0.046731	4.402725
227.184860	6641.019550	15.126618	-0.046701	4.400176
227.070135	6633.045032	15.131623	-0.046674	4.397621
227.174636	6625.011076	15.136627	-0.046688	4.395047
227.127849	6616.982466	15.141632	-0.046674	4.392472
227.319342	6608.967066	15.146637	-0.046705	4.389901
227.233223	6600.993282	15.151642	-0.046684	4.387340
227.014271	6592.969253	15.156647	-0.046638	4.384761
226.859186	6585.036268	15.161651	-0.046604	4.382210
226.919133	6577.007008	15.166656	-0.046610	4.379628
226.862403	6569.049597	15.171661	-0.046594	4.377067
226.723698	6561.010206	15.176666	-0.046563	4.374477
226.670589	6552.991460	15.181671	-0.046548	4.371893
226.701937	6544.989429	15.186675	-0.046549	4.369313
226.646798	6536.974433	15.191680	-0.046533	4.366727
226.623759	6528.994532	15.196685	-0.046524	4.364151
226.693976	6521.025261	15.201690	-0.046532	4.361578
226.673145	6512.961072	15.206695	-0.046523	4.358971
226.467997	6505.042467	15.211699	-0.046479	4.356410
226.360161	6496.963624	15.216704	-0.046454	4.353795
226.404487	6488.861517	15.221709	-0.046457	4.351172
226.663978	6480.954471	15.226714	-0.046500	4.348612
226.434924	6472.927336	15.231719	-0.046453	4.346009
226.268502	6464.992328	15.236723	-0.046416	4.343434
226.042774	6456.980647	15.241728	-0.046369	4.340833
225.967216	6448.990842	15.246733	-0.046350	4.338238
226.055061	6440.992728	15.251738	-0.046361	4.335639
226.226486	6432.939962	15.256743	-0.046388	4.333023
226.166761	6424.969989	15.261747	-0.046372	4.330429
226.074245	6416.945142	15.266752	-0.046349	4.327817
226.119112	6408.927866	15.271757	-0.046353	4.325206
226.090090	6401.010938	15.276762	-0.046342	4.322625
225.974161	6392.923669	15.281767	-0.046315	4.319987
226.133038	6385.005355	15.286771	-0.046340	4.317405
225.909241	6376.928498	15.291776	-0.046293	4.314766
225.764893	6368.929345	15.296781	-0.046261	4.312152
225.901398	6360.913234	15.301786	-0.046281	4.309532
225.820690	6352.957667	15.306791	-0.046261	4.306930
225.877409	6344.922611	15.311795	-0.046266	4.304300
225.599614	6336.973886	15.316800	-0.046209	4.301695
225.598377	6328.932902	15.321805	-0.046204	4.299060
225.598772	6320.979627	15.326810	-0.046199	4.296452
225.236801	6312.933582	15.331815	-0.046126	4.293809
225.476851	6304.922365	15.336819	-0.046166	4.291181
225.289239	6296.896274	15.341824	-0.046126	4.288543
225.254860	6288.877985	15.346829	-0.046114	4.285907
225.187715	6280.962274	15.351834	-0.046097	4.283303
225.125123	6272.958356	15.356839	-0.046080	4.280668
225.159970	6264.959727	15.361843	-0.046081	4.278035
224.938325	6256.949010	15.366848	-0.046035	4.275393
224.983257	6248.875774	15.371853	-0.046038	4.272732
224.809824	6240.907922	15.376858	-0.046000	4.270101
224.703107	6232.861032	15.381863	-0.045975	4.267444
225.081002	6224.882753	15.386867	-0.046041	4.264812
225.016775	6216.919297	15.391872	-0.046023	4.262179
224.843337	6208.923185	15.396877	-0.045986	4.259533
224.695435	6200.951225	15.401882	-0.045953	4.256893
224.788638	6192.911659	15.406887	-0.045966	4.254232
224.493909	6184.935898	15.411891	-0.045906	4.251586
224.487356	6176.909168	15.416896	-0.045899	4.248925
224.592856	6168.896553	15.421901	-0.045914	4.246267
224.524901	6160.920157	15.426906	-0.045896	4.243618
224.448493	6152.918953	15.431911	-0.045876	4.240960
224.311814	6144.974299	15.436915	-0.045846	4.238318
224.258424	6136.938420	15.441920	-0.045831	4.235644
224.387297	6128.924844	15.446925	-0.045850	4.232978
224.415556	6120.922032	15.451930	-0.045850	4.230313
224.310500	6112.954415	15.456935	-0.045825	4.227657
224.282055	6104.924999	15.461939	-0.045814	4.224979
224.020992	6096.986215	15.466944	-0.045761	4.222328
224.014019	6088.937390	15.471949	-0.045754	4.219640
224.071096	6080.979577	15.476954	-0.045760	4.216982
224.008321	6072.915586	15.481959	-0.045743	4.214286
224.089710	6064.920478	15.486963	-0.045753	4.211612
223.890159	6056.907387	15.491968	-0.045711	4.208928
223.861896	6048.937974	15.496973	-0.045700	4.206258
223.650424	6040.984949	15.501978	-0.045656	4.203591
223.741582	6032.930772	15.506983	-0.045667	4.200890
223.697631	6024.997617	15.511987	-0.045654	4.198228
223.703697	6016.943388	15.516992	-0.045650	4.195523
223.724938	6008.857649	15.521997	-0.045649	4.192806
223.777053	6000.835559	15.527002	-0.045653	4.190109
223.422074	5992.850364	15.532007	-0.045582	4.187419
223.631537	5984.910456	15.537011	-0.045616	4.184748
223.317275	5976.961213	15.542016	-0.045552	4.182067
223.446106	5968.922045	15.547021	-0.045571	4.179358
223.426438	5960.944781	15.552026	-0.045562	4.176667
223.328930	5952.886510	15.557031	-0.045539	4.173946
223.162864	5944.894978	15.562035	-0.045503	4.171244
223.015928	5936.901588	15.567040	-0.045470	4.168541
223.026155	5928.863822	15.572045	-0.045467	4.165823
222.986640	5920.913234	15.577050	-0.045455	4.163132
222.935551	5912.886186	15.582055	-0.045440	4.160413
222.835891	5904.963717	15.587059	-0.045416	4.157727
222.826048	5896.933769	15.592064	-0.045409	4.155004
222.673766	5888.918669	15.597069	-0.045376	4.152282
222.677998	5880.886853	15.602074	-0.045371	4.149555
222.652351	5872.843925	15.607079	-0.045361	4.146822
222.762410	5864.868512	15.612083	-0.045377	4.144112
222.547854	5856.913534	15.617088	-0.045332	4.141403
222.435276	5848.894190	15.622093	-0.045306	4.138672
222.574979	5840.915066	15.627098	-0.045326	4.135955
222.424042	5832.867447	15.632103	-0.045293	4.133210
222.497844	5824.869200	15.637107	-0.045302	4.130483
222.461155	5816.874777	15.642112	-0.045290	4.127753
222.307144	5808.867146	15.647117	-0.045256	4.125016
222.376099	5800.958908	15.652122	-0.045264	4.122314
222.272763	5792.881573	15.657127	-0.045239	4.119550
222.358330	5784.957660	15.662131	-0.045250	4.116839
222.085775	5776.896582	15.667136	-0.045194	4.114075
222.030920	5768.860128	15.672141	-0.045179	4.111320
222.197541	5760.892567	15.677146	-0.045205	4.108590
221.863684	5752.845685	15.682151	-0.045137	4.105824
221.930564	5744.938940	15.687155	-0.045145	4.103110
221.760898	5736.920291	15.692160	-0.045108	4.100353
221.850393	5728.929735	15.697165	-0.045119	4.097606
221.707815	5720.926344	15.702170	-0.045088	4.094850
221.726342	5712.882213	15.707175	-0.045086	4.092081
221.900831	5704.897169	15.712179	-0.045113	4.089332
221.753225	5696.915691	15.717184	-0.045081	4.086578
221.708740	5688.955461	15.722189	-0.045067	4.083831
221.849873	5680.957040	15.727194	-0.045088	4.081071
221.615539	5672.956466	15.732199	-0.045039	4.078304
221.610889	5664.977438	15.737203	-0.045033	4.075545
221.617086	5656.923095	15.742208	-0.045029	4.072759
221.476466	5648.921715	15.747213	-0.044998	4.069987
221.531442	5640.920552	15.752218	-0.045003	4.067216
221.370756	5632.881478	15.757223	-0.044968	4.064427
221.283347	5624.991610	15.762227	-0.044947	4.061688
221.063087	5616.944501	15.767232	-0.044901	4.058892
221.164092	5608.958820	15.772237	-0.044914	4.056119
221.244721	5600.926449	15.777242	-0.044924	4.053328
220.968711	5592.931637	15.782247	-0.044867	4.050543
220.970994	5584.947716	15.787251	-0.044863	4.047764
220.929241	5576.903064	15.792256	-0.044850	4.044961
220.846781	5568.976768	15.797261	-0.044829	4.042196
220.705748	5560.973448	15.802266	-0.044798	4.039403
220.698852	5552.992310	15.807271	-0.044791	4.036617
220.734279	5544.910328	15.812275	-0.044793	4.033794
220.620209	5536.801206	15.817280	-0.044766	4.030958
220.497896	5528.883781	15.822285	-0.044738	4.028186
220.525359	5520.906455	15.827290	-0.044738	4.025394
220.531636	5512.926683	15.832295	-0.044734	4.022599
220.486386	5504.937822	15.837299	-0.044721	4.019798
220.401904	5496.945622	15.842304	-0.044700	4.016993
220.340746	5488.913552	15.847309	-0.044683	4.014173
220.249792	5480.906263	15.852314	-0.044661	4.011359
220.286918	5472.907756	15.857319	-0.044663	4.008548
220.431628	5464.942817	15.862323	-0.044685	4.005748
220.164806	5456.957734	15.867328	-0.044630	4.002933
220.112132	5448.911930	15.872333	-0.044615	4.000098
220.339364	5440.962634	15.877338	-0.044652	3.997299
220.038884	5432.900628	15.882343	-0.044591	3.994450
220.088302	5424.900855	15.887347	-0.044595	3.991627
219.925986	5416.885619	15.892352	-0.044560	3.988793
220.041423	5408.893246	15.897357	-0.044576	3.985970
219.913452	5400.953155	15.902362	-0.044547	3.983158
219.752205	5392.924201	15.907367	-0.044512	3.980313
219.891101	5384.981183	15.912371	-0.044533	3.977502
219.725793	5376.967447	15.917376	-0.044497	3.974658
219.412876	5368.985888	15.922381	-0.044433	3.971821
219.668031	5360.932973	15.927386	-0.044476	3.968966
219.666551	5352.916487	15.932391	-0.044470	3.966118
219.712443	5344.980734	15.937395	-0.044474	3.963297
219.580874	5337.005677	15.942400	-0.044444	3.960457
219.451714	5329.016127	15.947405	-0.044415	3.957610
219.363623	5321.029512	15.952410	-0.044393	3.954763
219.208320	5312.956576	15.957415	-0.044359	3.951882
219.314025	5304.952889	15.962419	-0.044374	3.949028
218.994746	5296.977625	15.967424	-0.044309	3.946174
219.010014	5288.966406	15.972429	-0.044307	3.943312
219.087754	5281.003286	15.977434	-0.044316	3.940465
218.973045	5272.994436	15.982439	-0.044290	3.937597
219.133639	5265.004723	15.987443	-0.044314	3.934739
218.923853	5256.974040	15.992448	-0.044270	3.931857
218.973580	5248.975419	15.997453	-0.044274	3.928989
218.934771	5241.002754	16.002458	-0.044262	3.926127
218.687869	5232.992624	16.007463	-0.044211	3.923245
218.893381	5225.014049	16.012467	-0.044244	3.920381
218.880631	5217.043716	16.017472	-0.044236	3.917514
218.608964	5209.005835	16.022477	-0.044181	3.914615
218.798398	5201.002234	16.027482	-0.044211	3.911735
218.827679	5192.954741	16.032487	-0.044211	3.908835
218.669633	5184.984364	16.037491	-0.044176	3.905956
218.510919	5177.032937	16.042496	-0.044142	3.903083
218.480041	5168.987466	16.047501	-0.044131	3.900175
218.441288	5161.051137	16.052506	-0.044118	3.897305
218.431963	5152.985444	16.057511	-0.044111	3.894386
218.437112	5144.991403	16.062515	-0.044107	3.891491
218.379772	5136.991132	16.067520	-0.044091	3.888591
218.129191	5128.969298	16.072525	-0.044040	3.885677
218.243495	5121.001147	16.077530	-0.044056	3.882787
217.933975	5112.999774	16.082535	-0.043993	3.879875
217.902043	5105.060854	16.087539	-0.043982	3.876988
217.665905	5096.954452	16.092544	-0.043933	3.874035
217.808601	5088.748910	16.097549	-0.043954	3.871051
217.811285	5080.897346	16.102554	-0.043949	3.868190
217.630151	5072.876747	16.107559	-0.043911	3.865263
217.827105	5064.963030	16.112563	-0.043942	3.862379
217.746973	5056.992618	16.117568	-0.043922	3.859467
217.598061	5049.017543	16.122573	-0.043889	3.856550
217.454428	5041.031212	16.127578	-0.043857	3.853627
217.384706	5032.998292	16.132583	-0.043839	3.850685
217.558937	5025.004794	16.137587	-0.043866	3.847761
217.391996	5016.978516	16.142592	-0.043830	3.844816
217.311018	5009.032758	16.147597	-0.043810	3.841900
217.095045	5001.070932	16.152602	-0.043765	3.838972
217.083943	4993.063759	16.157607	-0.043757	3.836031
217.008548	4985.042623	16.162611	-0.043738	3.833080
217.036696	4977.019258	16.167616	-0.043738	3.830128
216.908837	4969.024552	16.172621	-0.043709	3.827182
217.150925	4961.030086	16.177626	-0.043749	3.824241
217.095305	4953.085041	16.182631	-0.043734	3.821310
217.100689	4945.083409	16.187635	-0.043730	3.818357
216.905905	4937.108019	16.192640	-0.043688	3.815407
216.796748	4929.099295	16.197645	-0.043663	3.812444
216.979771	4921.071371	16.202650	-0.043692	3.809478
216.695536	4913.091303	16.207655	-0.043633	3.806517
216.691399	4905.107864	16.212659	-0.043628	3.803559
216.701111	4897.112154	16.217664	-0.043624	3.800595
216.673437	4889.146760	16.222669	-0.043614	3.797638
216.290346	4881.132195	16.227674	-0.043537	3.794653
216.237761	4873.060786	16.232679	-0.043522	3.791652
216.440808	4865.067792	16.237683	-0.043555	3.788683
216.181872	4857.067567	16.242688	-0.043502	3.785699
216.162111	4849.094582	16.247693	-0.043493	3.782728
216.236265	4841.115519	16.252698	-0.043502	3.779755
216.122462	4833.087168	16.257703	-0.043475	3.776757
216.055922	4825.118370	16.262707	-0.043458	3.773779
215.948844	4817.069854	16.267712	-0.043433	3.770769
215.960527	4809.094824	16.272717	-0.043430	3.767786
215.964074	4801.124108	16.277722	-0.043425	3.764802
215.801961	4793.133239	16.282727	-0.043390	3.761805
215.893433	4785.131526	16.287731	-0.043402	3.758807
215.770066	4777.141126	16.292736	-0.043374	3.755805
215.708398	4769.097671	16.297741	-0.043357	3.752783
215.793980	4761.087273	16.302746	-0.043368	3.749775
215.703314	4753.095100	16.307751	-0.043346	3.746766
215.505495	4745.148428	16.312755	-0.043304	3.743770
215.471524	4737.163134	16.317760	-0.043292	3.740761
215.446962	4729.154727	16.322765	-0.043282	3.737741
215.599368	4721.168922	16.327770	-0.043306	3.734731
215.554672	4713.134225	16.332775	-0.043292	3.731695
215.358770	4705.141295	16.337779	-0.043251	3.728669
215.347332	4697.155562	16.342784	-0.043243	3.725648
215.129455	4689.198583	16.347789	-0.043198	3.722630
215.358604	4681.195605	16.352794	-0.043235	3.719604
215.307535	4673.230239	16.357799	-0.043220	3.716582
215.187038	4665.175540	16.362803	-0.043193	3.713522
215.093237	4657.091306	16.367808	-0.043170	3.710449
214.973924	4649.147640	16.372813	-0.043143	3.707426
215.081160	4641.155570	16.377818	-0.043158	3.704388
214.926123	4633.193696	16.382823	-0.043124	3.701353
215.047119	4625.192509	16.387827	-0.043141	3.698307
214.800035	4617.181950	16.392832	-0.043090	3.695245
214.734240	4609.187459	16.397837	-0.043072	3.692192
214.771040	4601.222244	16.402842	-0.043074	3.689150
214.646062	4593.220440	16.407847	-0.043046	3.686087
214.615690	4585.254943	16.412851	-0.043035	3.683038
214.470425	4577.248311	16.417856	-0.043003	3.679968
214.550704	4569.270806	16.422861	-0.043012	3.676912
214.617865	4561.269057	16.427866	-0.043020	3.673844
214.577483	4553.221866	16.432871	-0.043007	3.670753
214.570872	4545.249040	16.437875	-0.043001	3.667689
214.444524	4537.219576	16.442880	-0.042972	3.664598
214.300156	4529.271136	16.447885	-0.042940	3.661535
214.339441	4521.261847	16.452890	-0.042942	3.658450
214.326226	4513.252360	16.457895	-0.042935	3.655362
214.222251	4505.245348	16.462899	-0.042910	3.652269
214.112474	4497.234256	16.467904	-0.042884	3.649172
213.843629	4489.265986	16.472909	-0.042829	3.646085
213.746808	4481.303212	16.477914	-0.042806	3.643001
213.676136	4473.264828	16.482919	-0.042788	3.639887
213.628159	4465.329220	16.487923	-0.042774	3.636810
213.511168	4457.283668	16.492928	-0.042747	3.633686
213.588040	4449.224339	16.497933	-0.042756	3.630559
213.655652	4441.265737	16.502938	-0.042763	3.627469
213.685719	4433.210600	16.507943	-0.042764	3.624337
213.598585	4425.302150	16.512947	-0.042742	3.621257
213.581836	4417.306590	16.517952	-0.042734	3.618142
213.733042	4409.282042	16.522957	-0.042757	3.615017
213.515752	4401.329681	16.527962	-0.042711	3.611908
213.316061	4393.303917	16.532967	-0.042669	3.608768
213.348214	4385.341353	16.537971	-0.042670	3.605656
213.351456	4377.360601	16.542976	-0.042665	3.602534
213.119873	4369.337459	16.547981	-0.042617	3.599386
213.181240	4361.419030	16.552986	-0.042623	3.596284
212.948994	4353.398099	16.557991	-0.042575	3.593131
213.044472	4345.359845	16.562995	-0.042588	3.589978
212.944964	4337.386420	16.568000	-0.042564	3.586842
212.797231	4329.381469	16.573005	-0.042531	3.583689
212.854834	4321.430513	16.578010	-0.042537	3.580561
212.828665	4313.409438	16.583015	-0.042527	3.577400
212.879312	4305.417542	16.588019	-0.042531	3.574250
212.650646	4297.414438	16.593024	-0.042483	3.571084
212.526853	4289.410819	16.598029	-0.042455	3.567919
212.618182	4281.427691	16.603034	-0.042467	3.564765
212.571487	4273.462593	16.608039	-0.042453	3.561612
212.424181	4265.470284	16.613043	-0.042421	3.558441
212.218565	4257.468255	16.618048	-0.042377	3.555263
212.306394	4249.339926	16.623053	-0.042388	3.552040
212.197003	4241.375898	16.628058	-0.042363	3.548874
212.125892	4233.358073	16.633063	-0.042344	3.545684
212.034021	4225.421999	16.638067	-0.042322	3.542524
212.098743	4217.420918	16.643072	-0.042329	3.539340
211.851171	4209.456086	16.648077	-0.042278	3.536157
211.891498	4201.467351	16.653082	-0.042280	3.532971
211.920507	4193.403834	16.658087	-0.042280	3.529752
211.918485	4185.489781	16.663091	-0.042275	3.526589
212.003783	4177.470865	16.668096	-0.042286	3.523384
211.877556	4169.481630	16.673101	-0.042257	3.520181
211.762978	4161.569690	16.678106	-0.042231	3.517006
211.635387	4153.513480	16.683111	-0.042202	3.513771
211.668137	4145.492808	16.688115	-0.042203	3.510551
211.672229	4137.501111	16.693120	-0.042198	3.507340
211.695887	4129.510566	16.698125	-0.042197	3.504126
211.597786	4121.569355	16.703130	-0.042174	3.500926
211.508934	4113.541813	16.708135	-0.042152	3.497688
211.415792	4105.564635	16.713139	-0.042130	3.494467
211.268788	4097.579751	16.718144	-0.042097	3.491239
211.382788	4089.556370	16.723149	-0.042113	3.488000
211.325801	4081.590098	16.728154	-0.042098	3.484776
211.124206	4073.625672	16.733159	-0.042055	3.481545
211.208118	4065.628466	16.738163	-0.042065	3.478307
211.198173	4057.627644	16.743168	-0.042058	3.475061
210.933292	4049.574616	16.748173	-0.042004	3.471783
210.896769	4041.592538	16.753178	-0.041992	3.468538
210.878729	4033.584257	16.758183	-0.041983	3.465280
210.960470	4025.604664	16.763187	-0.041993	3.462034
210.707670	4017.647860	16.768192	-0.041941	3.458783
210.927242	4009.600260	16.773197	-0.041977	3.455507
210.750740	4001.641015	16.778202	-0.041939	3.452252
210.671589	3993.611259	16.783207	-0.041919	3.448967
210.696100	3985.620467	16.788211	-0.041918	3.445699
210.549126	3977.675551	16.793216	-0.041886	3.442441
210.463703	3969.641100	16.798221	-0.041865	3.439145
210.550834	3961.712138	16.803226	-0.041876	3.435895
210.460086	3953.679796	16.808231	-0.041854	3.432594
210.419647	3945.656422	16.813235	-0.041841	3.429294
210.207740	3937.707963	16.818240	-0.041797	3.426017
210.164265	3929.691219	16.823245	-0.041783	3.422714
210.149849	3921.725260	16.828250	-0.041776	3.419429
209.909070	3913.762240	16.833255	-0.041726	3.416135
209.866827	3905.752786	16.838259	-0.041713	3.412826
210.054353	3897.676941	16.843264	-0.041742	3.409493
210.031708	3889.734235	16.848269	-0.041733	3.406205
209.935112	3881.793332	16.853274	-0.041710	3.402913
209.803179	3873.769050	16.858279	-0.041680	3.399581
209.731815	3865.831076	16.863283	-0.041662	3.396284
209.636056	3857.778216	16.868288	-0.041639	3.392935
209.805858	3849.672720	16.873293	-0.041665	3.389570
209.774481	3841.788579	16.878298	-0.041654	3.386287
209.366506	3833.791201	16.883303	-0.041573	3.382940
209.330129	3825.812311	16.888307	-0.041561	3.379611
209.335694	3817.863898	16.893312	-0.041557	3.376292
209.251029	3809.811525	16.898317	-0.041536	3.372924
209.404949	3801.816235	16.903322	-0.041560	3.369585
209.366747	3793.842265	16.908327	-0.041547	3.366244
209.220380	3785.877323	16.913331	-0.041515	3.362900
209.144397	3777.866731	16.918336	-0.041496	3.359536
209.114327	3769.901106	16.923341	-0.041485	3.356189
209.193815	3761.899102	16.928346	-0.041494	3.352828
209.090219	3753.862362	16.933351	-0.041470	3.349442
209.051491	3745.885209	16.938355	-0.041458	3.346080
209.093734	3737.903137	16.943360	-0.041460	3.342715
209.001802	3729.917122	16.948365	-0.041438	3.339341
209.046150	3721.962034	16.953370	-0.041441	3.335981
208.926919	3713.920080	16.958375	-0.041414	3.332575
208.620849	3705.928591	16.963379	-0.041352	3.329179
208.679257	3697.975939	16.968384	-0.041357	3.325811
208.684317	3689.939679	16.973389	-0.041353	3.322401
208.709618	3682.007596	16.978394	-0.041353	3.319033
208.472021	3674.029755	16.983399	-0.041303	3.315632
208.658384	3665.990361	16.988403	-0.041333	3.312218
208.440742	3658.011190	16.993408	-0.041287	3.308810
208.225542	3650.007937	16.998413	-0.041242	3.305389
208.233347	3642.063338	17.003418	-0.041238	3.301997
208.185973	3634.037648	17.008423	-0.041224	3.298566
208.157520	3626.047817	17.013427	-0.041214	3.295146
208.085720	3618.058532	17.018432	-0.041195	3.291722
207.930604	3610.055986	17.023437	-0.041161	3.288286
208.114338	3602.060395	17.028442	-0.041190	3.284861
207.883039	3594.117121	17.033447	-0.041142	3.281440
207.722858	3586.143151	17.038451	-0.041107	3.278004
207.632689	3578.143720	17.043456	-0.041085	3.274557
207.794623	3570.085654	17.048461	-0.041110	3.271091
207.830855	3562.132864	17.053466	-0.041112	3.267661
207.508064	3554.150412	17.058471	-0.041047	3.264201
207.577630	3546.153644	17.063475	-0.041054	3.260747
207.559906	3538.193518	17.068480	-0.041046	3.257301
207.392232	3530.197281	17.073485	-0.041010	3.253830
207.425878	3522.163768	17.078490	-0.041011	3.250347
207.571114	3514.168076	17.083495	-0.041033	3.246881
207.425382	3506.197730	17.088499	-0.041000	3.243411
207.504240	3498.225918	17.093504	-0.041010	3.239946
207.352928	3490.273960	17.098509	-0.040977	3.236476
207.119361	3482.278872	17.103514	-0.040928	3.232980
207.036130	3474.202036	17.108519	-0.040907	3.229451
207.082390	3466.236209	17.113523	-0.040911	3.225972
207.125252	3458.249318	17.118528	-0.040914	3.222480
206.833717	3450.259004	17.123533	-0.040854	3.218968
206.929282	3442.311592	17.128538	-0.040867	3.215488
206.967585	3434.309890	17.133543	-0.040869	3.211978
206.716712	3426.300211	17.138547	-0.040817	3.208448
206.600883	3418.307969	17.143552	-0.040790	3.204927
206.752709	3410.345946	17.148557	-0.040813	3.201428
206.671525	3402.399134	17.153562	-0.040793	3.197921
206.563537	3394.371014	17.158567	-0.040768	3.194373
206.595993	3386.351883	17.163571	-0.040769	3.190832
206.563047	3378.384581	17.168576	-0.040757	3.187307
206.454316	3370.385458	17.173581	-0.040732	3.183760
206.536786	3362.399470	17.178586	-0.040742	3.180223
206.285947	3354.443850	17.183591	-0.040690	3.176682
206.342228	3346.428993	17.188595	-0.040696	3.173124
206.293764	3338.430414	17.193600	-0.040681	3.169564
206.109681	3330.477799	17.198605	-0.040642	3.166015
205.968877	3322.510400	17.203610	-0.040611	3.162457
205.762353	3314.528363	17.208615	-0.040567	3.158886
206.054601	3306.510383	17.213619	-0.040616	3.155316
205.909387	3298.496582	17.218624	-0.040584	3.151725
205.687993	3290.488984	17.223629	-0.040538	3.148129
205.775532	3282.507018	17.228634	-0.040549	3.144555
205.651340	3274.550001	17.233639	-0.040521	3.140978
205.618820	3266.558379	17.238643	-0.040509	3.137385
205.517875	3258.606252	17.243648	-0.040486	3.133804
205.519692	3250.549901	17.248653	-0.040481	3.130175
205.664294	3242.593259	17.253658	-0.040503	3.126594
205.411935	3234.615195	17.258663	-0.040450	3.122981
205.393936	3226.643931	17.263667	-0.040442	3.119378
205.601000	3218.667083	17.268672	-0.040475	3.115778
205.480304	3210.635597	17.273677	-0.040448	3.112134
205.435618	3202.654146	17.278682	-0.040434	3.108512
205.330246	3194.657172	17.283687	-0.040409	3.104876
205.146786	3186.717260	17.288691	-0.040370	3.101259
204.970688	3178.758546	17.293696	-0.040332	3.097628
204.985068	3170.709280	17.298701	-0.040330	3.093961
204.965727	3162.743398	17.303706	-0.040321	3.090326
204.944259	3154.763889	17.308711	-0.040312	3.086681
204.908003	3146.776894	17.313715	-0.040300	3.083027
205.202623	3138.758334	17.318720	-0.040350	3.079369
204.904051	3130.825088	17.323725	-0.040289	3.075719
205.027385	3122.751036	17.328730	-0.040307	3.072019
204.808291	3114.748742	17.333735	-0.040261	3.068332
204.677263	3106.776344	17.338739	-0.040231	3.064659
204.737717	3098.845454	17.343744	-0.040237	3.061009
204.777631	3090.840171	17.348749	-0.040240	3.057319
204.834849	3082.875869	17.353754	-0.040245	3.053645
204.499615	3074.874462	17.358759	-0.040178	3.049930
204.355970	3066.932650	17.363763	-0.040146	3.046248
204.351516	3058.961217	17.368768	-0.040140	3.042554
204.199891	3050.960233	17.373773	-0.040106	3.038835
204.187871	3042.983525	17.378778	-0.040099	3.035129
204.097957	3034.982398	17.383783	-0.040077	3.031403
204.056032	3026.986827	17.388787	-0.040064	3.027678
204.035565	3019.002228	17.393792	-0.040055	3.023955
203.930709	3011.022260	17.398797	-0.040030	3.020224
203.853728	3003.087338	17.403802	-0.040011	3.016512
203.870854	2995.047009	17.408807	-0.040009	3.012750
203.923320	2987.025653	17.413811	-0.040014	3.008995
203.850760	2979.070014	17.418816	-0.039995	3.005259
203.707926	2971.102493	17.423821	-0.039963	3.001509
203.695633	2963.155091	17.428826	-0.039956	2.997771
203.750008	2955.142307	17.433831	-0.039961	2.994001
203.614310	2947.112103	17.438835	-0.039930	2.990208
203.430445	2939.171959	17.443840	-0.039891	2.986450
203.271432	2931.178534	17.448845	-0.039856	2.982664
203.575469	2923.194089	17.453850	-0.039908	2.978900
203.499299	2915.237151	17.458855	-0.039888	2.975126
203.263676	2907.245607	17.463859	-0.039839	2.971322
203.108843	2899.262982	17.468864	-0.039805	2.967521
203.267446	2891.258312	17.473869	-0.039830	2.963721
203.280238	2883.307027	17.478874	-0.039827	2.959935
203.043214	2875.360129	17.483879	-0.039778	2.956133
203.008394	2867.333147	17.488883	-0.039766	2.952297
202.849360	2859.360717	17.493888	-0.039731	2.948477
202.817172	2851.330222	17.498893	-0.039720	2.944630
202.908850	2843.400916	17.503898	-0.039732	2.940834
202.814116	2835.407184	17.508903	-0.039709	2.936992
202.659607	2827.429179	17.513907	-0.039675	2.933149
202.955753	2819.401505	17.518912	-0.039725	2.929300
202.705546	2811.452376	17.523917	-0.039674	2.925456
202.630541	2803.503043	17.528922	-0.039655	2.921616
202.690534	2795.509359	17.533927	-0.039661	2.917757
202.689723	2787.503886	17.538931	-0.039655	2.913883
202.460269	2779.474991	17.543936	-0.039607	2.909981
202.047840	2771.537621	17.548941	-0.039525	2.906108
202.255326	2763.541270	17.553946	-0.039559	2.902235
202.369869	2755.561283	17.558951	-0.039575	2.898359
201.999261	2747.621363	17.563955	-0.039501	2.894472
201.922165	2739.599581	17.568960	-0.039481	2.890555
202.026065	2731.610095	17.573965	-0.039496	2.886658
202.181796	2723.632581	17.578970	-0.039519	2.882765
201.989228	2715.689996	17.583975	-0.039479	2.878865
201.964141	2707.711556	17.588979	-0.039469	2.874951
201.932413	2699.729490	17.593984	-0.039458	2.871029
201.633000	2691.725580	17.598989	-0.039397	2.867077
201.780549	2683.754213	17.603994	-0.039419	2.863160
201.803731	2675.783639	17.608999	-0.039418	2.859231
201.634214	2667.823632	17.614003	-0.039382	2.855291
201.641908	2659.831964	17.619008	-0.039378	2.851339
201.652325	2651.825859	17.624013	-0.039375	2.847376
201.418344	2643.896359	17.629018	-0.039326	2.843431
201.202528	2635.930688	17.634023	-0.039281	2.839463
201.354506	2627.958893	17.639027	-0.039304	2.835508
201.432603	2619.908815	17.644032	-0.039313	2.831504
201.224922	2611.935239	17.649037	-0.039269	2.827516
201.088030	2603.976800	17.654042	-0.039239	2.823535
201.012362	2595.980849	17.659047	-0.039219	2.819532
201.102752	2588.018981	17.664051	-0.039231	2.815550
201.116397	2580.029865	17.669056	-0.039229	2.811544
200.890977	2572.034919	17.674061	-0.039181	2.807516
201.013011	2564.092768	17.679066	-0.039199	2.803529
200.919429	2556.106843	17.684071	-0.039176	2.799502
200.768796	2548.181742	17.689075	-0.039143	2.795496
200.705040	2540.158569	17.694080	-0.039126	2.791440
200.519609	2532.160600	17.699085	-0.039087	2.787384
200.706237	2524.195163	17.704090	-0.039116	2.783360
200.546558	2516.223668	17.709095	-0.039081	2.779306
200.406037	2508.272707	17.714099	-0.039050	2.775259
200.426165	2500.280312	17.719104	-0.039049	2.771193
200.373740	2492.279347	17.724109	-0.039034	2.767114
200.471148	2484.329501	17.729114	-0.039047	2.763063
200.180551	2476.378217	17.734119	-0.038987	2.758982
200.045576	2468.410800	17.739123	-0.038957	2.754896
200.314802	2460.312095	17.744128	-0.039002	2.750762
200.051357	2452.350266	17.749133	-0.038948	2.746659
199.973215	2444.399207	17.754138	-0.038928	2.742566
200.007308	2436.424956	17.759143	-0.038929	2.738463
200.025091	2428.451261	17.764147	-0.038928	2.734352
199.646089	2420.522178	17.769152	-0.038852	2.730234
199.488228	2412.532513	17.774157	-0.038817	2.726092
199.584898	2404.557871	17.779162	-0.038830	2.721968
199.466046	2396.602343	17.784167	-0.038803	2.717833
199.378034	2388.622876	17.789171	-0.038781	2.713682
199.335122	2380.632281	17.794176	-0.038768	2.709521
199.203144	2372.658081	17.799181	-0.038739	2.705357
199.194646	2364.696936	17.804186	-0.038732	2.701201
199.215796	2356.734333	17.809191	-0.038731	2.697040
199.237280	2348.710085	17.814195	-0.038730	2.692840
199.075092	2340.759179	17.819200	-0.038694	2.688660
199.306419	2332.755331	17.824205	-0.038732	2.684471
199.423226	2324.816849	17.829210	-0.038749	2.680302
199.183568	2316.877632	17.834215	-0.038699	2.676104
199.194377	2308.853189	17.839219	-0.038696	2.671870
199.029000	2300.907750	17.844224	-0.038660	2.667660
198.904400	2292.910458	17.849229	-0.038632	2.663419
198.849151	2284.963990	17.854234	-0.038616	2.659202
198.812370	2276.992065	17.859239	-0.038604	2.654966
198.818914	2268.999718	17.864243	-0.038600	2.650715
198.676678	2261.048385	17.869248	-0.038569	2.646470
198.412813	2253.086832	17.874253	-0.038514	2.642204
198.482737	2245.129907	17.879258	-0.038522	2.637956
198.417427	2237.146479	17.884263	-0.038505	2.633678
198.426394	2229.135478	17.889267	-0.038501	2.629382
198.400398	2221.192117	17.894272	-0.038491	2.625114
198.242479	2213.230470	17.899277	-0.038457	2.620821
198.287138	2205.272762	17.904282	-0.038460	2.616536
198.384935	2197.256732	17.909287	-0.038473	2.612215
198.149197	2189.301729	17.914291	-0.038424	2.607899
198.035564	2181.352023	17.919296	-0.038398	2.603586
197.928186	2173.396658	17.924301	-0.038373	2.599264
197.913287	2165.449058	17.929306	-0.038365	2.594944
197.838992	2157.274532	17.934311	-0.038346	2.590490
197.832246	2149.299026	17.939315	-0.038339	2.586141
197.777675	2141.391203	17.944320	-0.038324	2.581819
197.553847	2133.457770	17.949325	-0.038277	2.577464
197.356994	2125.515977	17.954330	-0.038236	2.573099
197.318260	2117.544250	17.959335	-0.038223	2.568720
197.273730	2109.567008	17.964339	-0.038210	2.564331
197.428800	2101.617277	17.969344	-0.038233	2.559963
197.205562	2093.680035	17.974349	-0.038187	2.555569
197.225280	2085.692449	17.979354	-0.038185	2.551156
197.338881	2077.700541	17.984359	-0.038201	2.546739
197.088615	2069.760854	17.989363	-0.038150	2.542318
197.197405	2061.800309	17.994368	-0.038165	2.537903
197.013713	2053.833148	17.999373	-0.038125	2.533456
197.079082	2045.845445	18.004378	-0.038132	2.529008
197.188544	2037.872249	18.009383	-0.038148	2.524563
196.951064	2029.950819	18.014387	-0.038098	2.520114
197.038600	2021.992318	18.019392	-0.038109	2.515660
196.737588	2014.007545	18.024397	-0.038048	2.511155
196.862644	2006.017617	18.029402	-0.038066	2.506670
196.708794	1998.064873	18.034407	-0.038033	2.502177
196.296833	1990.143544	18.039411	-0.037951	2.497676
196.558345	1982.142165	18.044416	-0.037994	2.493170
196.466077	1974.158529	18.049421	-0.037972	2.488640
196.457599	1966.191521	18.054426	-0.037965	2.484118
196.455541	1958.254094	18.059431	-0.037960	2.479604
196.265029	1950.319228	18.064435	-0.037919	2.475070
196.207157	1942.347841	18.069440	-0.037903	2.470516
196.148033	1934.355884	18.074445	-0.037887	2.465942
196.246320	1926.398228	18.079450	-0.037900	2.461391
196.287873	1918.440909	18.084455	-0.037903	2.456828
196.124757	1910.478248	18.089459	-0.037867	2.452238
196.114210	1902.526263	18.094464	-0.037860	2.447656
195.940411	1894.573069	18.099469	-0.037823	2.443053
195.801173	1886.633382	18.104474	-0.037792	2.438452
195.594813	1878.664581	18.109479	-0.037748	2.433820
195.489299	1870.633000	18.114483	-0.037723	2.429150
195.530222	1862.664866	18.119488	-0.037726	2.424519
195.193663	1854.742648	18.124493	-0.037658	2.419877
195.335013	1846.775915	18.129498	-0.037679	2.415238
195.394471	1838.800343	18.134503	-0.037685	2.410578
195.068692	1830.855737	18.139507	-0.037619	2.405896
195.236351	1822.905675	18.144512	-0.037646	2.401241
195.253520	1814.939035	18.149517	-0.037644	2.396556
195.036477	1806.998348	18.154522	-0.037598	2.391858
194.922260	1799.046961	18.159527	-0.037572	2.387153
194.930876	1791.076411	18.164531	-0.037568	2.382437
194.983517	1783.128608	18.169536	-0.037573	2.377728
194.786249	1775.170507	18.174541	-0.037531	2.372984
194.798023	1767.199522	18.179546	-0.037528	2.368239
194.816367	1759.237856	18.184551	-0.037526	2.363491
194.730790	1751.292626	18.189555	-0.037505	2.358735
194.798847	1743.345306	18.194560	-0.037513	2.353981
194.521765	1735.368719	18.199565	-0.037456	2.349171
194.492175	1727.411658	18.204570	-0.037445	2.344383
194.467890	1719.469881	18.209575	-0.037436	2.339595
194.399347	1711.523268	18.214579	-0.037418	2.334791
194.394062	1703.553254	18.219584	-0.037412	2.329968
194.201265	1695.609091	18.224589	-0.037371	2.325135
194.274321	1687.659391	18.229594	-0.037379	2.320311
194.159479	1679.729311	18.234599	-0.037353	2.315472
193.916720	1671.770512	18.239603	-0.037302	2.310596
194.027712	1663.798285	18.244608	-0.037318	2.305730
194.006299	1655.836797	18.249613	-0.037309	2.300850
193.900158	1647.905880	18.254618	-0.037284	2.295971
193.852331	1639.953701	18.259623	-0.037270	2.291073
193.920212	1631.970486	18.264627	-0.037277	2.286156
193.969210	1624.038280	18.269632	-0.037281	2.281258
193.645905	1616.127949	18.274637	-0.037216	2.276331
193.430406	1608.146424	18.279642	-0.037171	2.271358
193.394496	1600.165141	18.284647	-0.037159	2.266390
193.460057	1592.186285	18.289651	-0.037166	2.261421
193.502717	1584.253044	18.294656	-0.037169	2.256468
193.435371	1576.282519	18.299661	-0.037151	2.251471
193.408949	1568.348614	18.304666	-0.037141	2.246490
193.213633	1560.435307	18.309671	-0.037100	2.241495
193.084619	1552.505016	18.314675	-0.037071	2.236485
193.009605	1544.569713	18.319680	-0.037052	2.231465
193.013501	1536.589044	18.324685	-0.037047	2.226411
193.065307	1528.640144	18.329690	-0.037052	2.221371
193.098599	1520.689285	18.334695	-0.037053	2.216316
192.920234	1512.745714	18.339699	-0.037014	2.211236
192.955590	1504.811133	18.344704	-0.037016	2.206169
192.903799	1496.857621	18.349709	-0.037001	2.201070
192.674220	1488.969296	18.354714	-0.036953	2.195984
192.471726	1481.014631	18.359719	-0.036910	2.190847
192.370675	1473.044316	18.364723	-0.036886	2.185697
192.366606	1465.120080	18.369728	-0.036881	2.180573
192.208601	1457.171846	18.374733	-0.036846	2.175408
192.252031	1449.213453	18.379738	-0.036849	2.170242
192.157186	1441.258937	18.384743	-0.036826	2.165054
192.172411	1433.327427	18.389747	-0.036824	2.159878
192.133579	1425.406179	18.394752	-0.036812	2.154691
192.119658	1417.426283	18.399757	-0.036804	2.149456
192.083418	1409.501740	18.404762	-0.036792	2.144243
191.865465	1401.600065	18.409767	-0.036746	2.139014
191.958493	1393.621752	18.414771	-0.036758	2.133752
192.120867	1385.666245	18.419776	-0.036784	2.128498
191.660707	1377.776902	18.424781	-0.036693	2.123216
191.604235	1369.872970	18.429786	-0.036677	2.117949
191.609694	1361.887493	18.434791	-0.036673	2.112621
191.465845	1353.910396	18.439795	-0.036641	2.107271
191.393989	1345.997153	18.444800	-0.036623	2.101956
191.407628	1338.050988	18.449805	-0.036620	2.096615
191.254110	1330.126869	18.454810	-0.036586	2.091258
191.113427	1322.210902	18.459815	-0.036555	2.085894
191.068410	1314.275461	18.464819	-0.036542	2.080513
191.273920	1306.334617	18.469824	-0.036575	2.075139
191.042527	1298.403063	18.474829	-0.036527	2.069713
190.919473	1290.487819	18.479834	-0.036499	2.064296
190.962307	1282.561418	18.484839	-0.036501	2.058873
191.021742	1274.603455	18.489843	-0.036507	2.053416
190.975691	1266.679104	18.494848	-0.036494	2.047956
190.798814	1258.774554	18.499853	-0.036456	2.042483
190.658700	1250.868105	18.504858	-0.036424	2.036997
190.692901	1242.911993	18.509863	-0.036426	2.031480
190.518745	1234.978365	18.514867	-0.036388	2.025942
190.464864	1227.075375	18.519872	-0.036373	2.020422
190.267547	1219.157491	18.524877	-0.036331	2.014862
190.403869	1211.186215	18.529882	-0.036351	2.009284
190.359547	1203.265707	18.534887	-0.036338	2.003707
189.980348	1195.399935	18.539891	-0.036262	1.998118
189.959063	1187.473082	18.544896	-0.036253	1.992508
189.978482	1179.507342	18.549901	-0.036252	1.986858
190.202808	1171.564800	18.554906	-0.036288	1.981231
189.869821	1163.703709	18.559911	-0.036221	1.975587
189.749001	1155.760229	18.564915	-0.036194	1.969890
189.864606	1147.832246	18.569920	-0.036210	1.964213
189.699821	1139.945867	18.574925	-0.036174	1.958519
189.588299	1132.014511	18.579930	-0.036149	1.952782
189.683106	1124.040459	18.584935	-0.036161	1.947019
189.628756	1116.114255	18.589939	-0.036146	1.941258
189.386103	1108.252345	18.594944	-0.036096	1.935506
189.302264	1100.311948	18.599949	-0.036075	1.929697
189.344733	1092.392398	18.604954	-0.036078	1.923899
189.328761	1084.489361	18.609959	-0.036070	1.918090
189.245810	1076.564767	18.614963	-0.036049	1.912239
189.309723	1068.648965	18.619968	-0.036056	1.906394
189.136557	1060.754425	18.624973	-0.036018	1.900519
188.910545	1052.883631	18.629978	-0.035971	1.894638
188.903210	1044.960748	18.634983	-0.035965	1.888725
188.801549	1037.048484	18.639987	-0.035941	1.882790
188.809620	1029.162551	18.644992	-0.035937	1.876869
188.613124	1021.242065	18.649997	-0.035896	1.870880
188.947617	1013.261412	18.655002	-0.035953	1.864887
188.837777	1005.395639	18.660007	-0.035927	1.858910
188.564848	997.516276	18.665011	-0.035871	1.852885
188.575418	989.608648	18.670016	-0.035868	1.846851
188.561588	981.699824	18.675021	-0.035860	1.840794
188.441012	973.821241	18.680026	-0.035833	1.834728
188.256312	965.936393	18.685031	-0.035793	1.828629
188.165460	958.027439	18.690035	-0.035771	1.822502
188.172797	950.141417	18.695040	-0.035768	1.816384
187.834695	942.263229	18.700045	-0.035700	1.810210
188.056742	934.332115	18.705050	-0.035736	1.804041
187.895758	926.463950	18.710055	-0.035701	1.797853
187.954746	918.510414	18.715059	-0.035707	1.791604
187.968141	910.592791	18.720064	-0.035704	1.785356
187.887750	902.715243	18.725069	-0.035684	1.779106
187.487074	894.878207	18.730074	-0.035604	1.772826
187.614597	886.958238	18.735079	-0.035623	1.766524
187.553795	879.071617	18.740083	-0.035607	1.760202
187.527875	871.207499	18.745088	-0.035597	1.753880
187.329001	863.322827	18.750093	-0.035555	1.747497
187.251837	855.440152	18.755098	-0.035535	1.741107
187.106182	847.593722	18.760103	-0.035503	1.734714
187.078160	839.675286	18.765107	-0.035493	1.728254
187.066293	831.804642	18.770112	-0.035485	1.721811
187.144905	823.921868	18.775117	-0.035495	1.715346
186.619951	816.086309	18.780122	-0.035392	1.708816
186.570841	808.201205	18.785127	-0.035378	1.702283
186.701010	800.292553	18.790131	-0.035397	1.695728
186.746399	792.410705	18.795136	-0.035400	1.689159
186.566007	784.563718	18.800141	-0.035362	1.682564
186.598672	776.694393	18.805146	-0.035363	1.675952
186.396036	768.840399	18.810151	-0.035320	1.669295
186.243191	760.974856	18.815155	-0.035286	1.662609
186.438726	753.088192	18.820160	-0.035318	1.655925
186.175902	745.248489	18.825165	-0.035264	1.649191
185.907092	737.412000	18.830170	-0.035209	1.642432
185.899643	729.566442	18.835175	-0.035202	1.635673
186.032646	721.600601	18.840179	-0.035222	1.628801
185.967464	713.763721	18.845184	-0.035205	1.621984
185.766619	705.929556	18.850189	-0.035162	1.615122
185.623053	698.081232	18.855194	-0.035130	1.608227
185.804652	690.205403	18.860199	-0.035159	1.601323
185.432751	682.410660	18.865203	-0.035085	1.594383
185.287133	674.576026	18.870208	-0.035053	1.587409
185.323076	666.702088	18.875213	-0.035054	1.580395
185.202734	658.883855	18.880218	-0.035027	1.573378
185.000035	651.051519	18.885223	-0.034984	1.566304
184.967318	643.213258	18.890227	-0.034973	1.559217
185.223758	635.335967	18.895232	-0.035016	1.552106
184.959385	627.504708	18.900237	-0.034961	1.544926
184.818810	619.692524	18.905242	-0.034930	1.537749
184.868247	611.847939	18.910247	-0.034934	1.530537
184.648427	604.038348	18.915251	-0.034888	1.523282
184.455386	596.253551	18.920256	-0.034847	1.516020
184.336197	588.420256	18.925261	-0.034820	1.508688
184.358856	580.587820	18.930266	-0.034819	1.501344
184.337178	572.777052	18.935271	-0.034810	1.493977
184.343955	564.927608	18.940275	-0.034806	1.486541
184.127047	557.172943	18.945280	-0.034761	1.479123
183.848672	549.359714	18.950285	-0.034704	1.471601
183.849904	541.507738	18.955290	-0.034699	1.464048
184.000258	533.681808	18.960295	-0.034722	1.456505
183.797716	525.894454	18.965299	-0.034680	1.448904
183.575940	518.138211	18.970304	-0.034633	1.441289
183.605257	510.327343	18.975309	-0.034634	1.433622
183.595995	502.513253	18.980314	-0.034627	1.425903
183.559836	494.741424	18.985319	-0.034615	1.418180
183.427502	486.951373	18.990323	-0.034586	1.410381
183.481216	479.168520	18.995328	-0.034591	1.402576
183.318635	471.416102	19.000333	-0.034555	1.394723
182.975012	463.663452	19.005338	-0.034486	1.386793
183.010929	455.879257	19.010343	-0.034488	1.378851
182.873710	448.103839	19.015347	-0.034457	1.370842
182.798807	440.349818	19.020352	-0.034438	1.362818
182.477246	432.637192	19.025357	-0.034374	1.354748
182.475328	424.858193	19.030362	-0.034368	1.346615
182.309607	417.119845	19.035367	-0.034332	1.338447
182.276211	409.348217	19.040371	-0.034321	1.330216
182.376500	401.589612	19.045376	-0.034335	1.321973
182.229443	393.829255	19.050381	-0.034302	1.313631
182.174461	385.986268	19.055386	-0.034287	1.305163
182.145968	378.277584	19.060391	-0.034277	1.296790
182.043092	370.555308	19.065395	-0.034253	1.288335
181.938913	362.860937	19.070400	-0.034228	1.279855
181.783723	355.167617	19.075405	-0.034195	1.271309
181.617304	347.471373	19.080410	-0.034159	1.262700
181.429783	339.793615	19.085415	-0.034119	1.254049
181.282941	332.095286	19.090419	-0.034086	1.245322
181.271953	324.407774	19.095424	-0.034079	1.236572
180.948812	316.734879	19.100429	-0.034014	1.227715
180.621590	309.082919	19.105434	-0.033948	1.218818
180.699664	301.379870	19.110439	-0.033958	1.209875
180.357497	293.742420	19.115443	-0.033889	1.200859
180.413950	286.068014	19.120448	-0.033895	1.191812
180.300713	278.401669	19.125453	-0.033869	1.182670
180.223100	270.755979	19.130458	-0.033850	1.173489
180.037349	263.126334	19.135463	-0.033810	1.164233
179.646615	255.540103	19.140467	-0.033732	1.154913
179.352330	247.901202	19.145472	-0.033673	1.145472
178.959149	240.321646	19.150477	-0.033595	1.136005
178.591472	232.730974	19.155482	-0.033521	1.126450
178.380696	225.147888	19.160487	-0.033477	1.116857
178.025571	217.563588	19.165491	-0.033406	1.107147
177.685368	210.016444	19.170496	-0.033338	1.097403
177.332475	202.449301	19.175501	-0.033267	1.087542
177.043406	194.903447	19.180506	-0.033209	1.077633
176.551857	187.374414	19.185511	-0.033112	1.067608
175.991677	179.865307	19.190515	-0.033003	1.057498
175.796733	172.306167	19.195520	-0.032962	1.047308
175.504269	164.790700	19.200525	-0.032903	1.037055
174.970544	157.313173	19.205530	-0.032798	1.026693
174.543607	149.842098	19.210535	-0.032714	1.016261
173.945521	142.388242	19.215539	-0.032598	1.005702
173.617296	134.921599	19.220544	-0.032532	0.995080
173.254414	127.424062	19.225549	-0.032460	0.984289
172.863404	119.984148	19.230554	-0.032382	0.973455
172.325924	112.583584	19.235559	-0.032277	0.962520
171.760394	105.203386	19.240563	-0.032167	0.951481
171.310568	97.815847	19.245568	-0.032079	0.940332
171.062886	90.406587	19.250573	-0.032028	0.929070
170.470833	83.081513	19.255578	-0.031913	0.917706
170.060597	75.726696	19.260583	-0.031832	0.906202
169.563810	68.414185	19.265587	-0.031734	0.894593
168.845396	61.382953	19.270592	-0.031596	0.883219