Thu Mar 11 21:11:10 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.788230	0.132464	0.000000	0.000036	0.722083

0.712799	0.147908	0.005005	0.000050	0.722087
0.634136	0.159238	0.010010	0.000065	0.722082
0.710702	0.148809	0.015014	0.000051	0.722088
0.766828	0.075591	0.020019	0.000040	0.721964
0.559057	0.005527	0.025024	0.000079	0.721754
0.546410	0.004826	0.030029	0.000081	0.721748
0.415564	0.027197	0.035034	0.000105	0.721746
0.479830	0.019830	0.040038	0.000093	0.721754
0.554231	0.003112	0.045043	0.000080	0.721748
0.671401	-0.014787	0.050048	0.000058	0.721754
0.584681	-0.000273	0.055053	0.000074	0.721752
0.577550	-0.000368	0.060058	0.000075	0.721749
0.689546	-0.017942	0.065062	0.000054	0.721754
0.602158	-0.005294	0.070067	0.000070	0.721748
0.804803	-0.039010	0.075072	0.000033	0.721753
0.740420	-0.028156	0.080077	0.000045	0.721752
0.672996	-0.016800	0.085082	0.000057	0.721751
0.612207	-0.031644	0.090086	0.000068	0.721701
0.652140	-0.172414	0.095091	0.000061	0.721438
0.546846	-0.147962	0.100096	0.000080	0.721449
0.529135	-0.148157	0.105101	0.000084	0.721443
0.637404	-0.169515	0.110106	0.000063	0.721439
0.705096	-0.175351	0.115110	0.000051	0.721451
0.628539	-0.166893	0.120115	0.000065	0.721441
0.737423	-0.302195	0.125120	0.000045	0.721213
0.682429	-0.336384	0.130125	0.000055	0.721127
0.651633	-0.333970	0.135130	0.000061	0.721121
0.732937	-0.342431	0.140134	0.000045	0.721133
0.682712	-0.339215	0.145139	0.000055	0.721122
0.711966	-0.451241	0.150144	0.000049	0.720912
0.542187	-0.437603	0.155149	0.000081	0.720879
0.579168	-0.445194	0.160154	0.000074	0.720877
0.580521	-0.443109	0.165158	0.000074	0.720882
0.300117	-0.509235	0.170163	0.000126	0.720654
0.565652	-0.610223	0.175168	0.000076	0.720548
0.625043	-0.623827	0.180173	0.000065	0.720542
0.426014	-0.589508	0.185178	0.000102	0.720540
0.449479	-0.727884	0.190182	0.000098	0.720276
0.558310	-0.775339	0.195187	0.000078	0.720221
0.519712	-0.763248	0.200192	0.000085	0.720231
0.290408	-0.791971	0.205197	0.000127	0.720094
0.315382	-0.894447	0.210202	0.000123	0.719901
0.510132	-0.926253	0.215206	0.000086	0.719907
0.338100	-0.933220	0.220211	0.000118	0.719833
0.452058	-1.069169	0.225216	0.000097	0.719605
0.574024	-1.093715	0.230221	0.000075	0.719600
0.485996	-1.134116	0.235226	0.000091	0.719489
0.617062	-1.266249	0.240230	0.000067	0.719275
0.237481	-1.202382	0.245235	0.000137	0.719268
0.239924	-1.287913	0.250240	0.000137	0.719100
0.303391	-1.368429	0.255245	0.000125	0.718963
0.402935	-1.387913	0.260250	0.000106	0.718960
0.306572	-1.515053	0.265254	0.000124	0.718675
0.226837	-1.517277	0.270259	0.000139	0.718643
0.302697	-1.587859	0.275264	0.000125	0.718531
0.161952	-1.651515	0.280269	0.000151	0.718355
-0.067570	-1.611520	0.285274	0.000194	0.718354
0.242221	-1.821268	0.290278	0.000136	0.718049
0.371149	-1.859931	0.295283	0.000112	0.718018
0.212421	-1.930156	0.300288	0.000142	0.717823
0.243207	-1.994343	0.305293	0.000136	0.717707
0.094773	-2.037496	0.310298	0.000163	0.717570
0.154531	-2.139863	0.315302	0.000152	0.717389
-0.124440	-2.132501	0.320307	0.000204	0.717305
-0.295456	-2.209867	0.325312	0.000236	0.717092
-0.399536	-2.198168	0.330317	0.000255	0.717078
-1.111001	-2.233186	0.335322	0.000388	0.716759
-2.139381	-2.046508	0.340326	0.000579	0.716766
-2.446992	-2.061959	0.345331	0.000636	0.716627
-3.048516	-2.039981	0.350336	0.000748	0.716458
-2.942609	-2.061266	0.355341	0.000729	0.716453
-3.322663	-2.043403	0.360346	0.000799	0.716355
-3.999663	-2.030285	0.365350	0.000925	0.716142
-3.600633	-2.105715	0.370355	0.000851	0.716134
-3.852008	-2.056026	0.375360	0.000898	0.716143
-4.509818	-2.057557	0.380365	0.001020	0.715908
-4.555137	-2.060369	0.385370	0.001028	0.715887
-4.249540	-2.110608	0.390374	0.000972	0.715895
-4.658166	-2.101475	0.395379	0.001048	0.715769
-6.014775	-1.967193	0.400384	0.001300	0.715557
-5.404102	-2.076940	0.405389	0.001186	0.715555
-5.744791	-2.018783	0.410394	0.001250	0.715550
-5.965513	-1.989122	0.415398	0.001291	0.715531
-6.567793	-2.031834	0.420403	0.001403	0.715233
-6.524202	-2.037962	0.425408	0.001395	0.715237
-7.077528	-1.938223	0.430413	0.001498	0.715239
-6.851438	-1.980325	0.435418	0.001455	0.715236
-6.366479	-2.092782	0.440422	0.001365	0.715184
-7.520956	-2.024457	0.445427	0.001580	0.714912
-7.203865	-2.078130	0.450432	0.001521	0.714917
-7.692829	-1.991350	0.455437	0.001612	0.714917
-7.953062	-1.947403	0.460442	0.001660	0.714912
-7.574585	-2.010478	0.465446	0.001590	0.714921
-8.352790	-2.023165	0.470451	0.001735	0.714621
-8.172808	-2.058979	0.475456	0.001701	0.714613
-8.616394	-1.978316	0.480461	0.001784	0.714617
-8.777004	-1.951447	0.485466	0.001813	0.714613
-8.238345	-2.044085	0.490470	0.001713	0.714620
-8.623593	-2.023739	0.495475	0.001785	0.714524
-9.689314	-1.955249	0.500480	0.001983	0.714283
-9.049322	-2.068026	0.505485	0.001864	0.714286
-9.569546	-1.978423	0.510490	0.001961	0.714280
-9.415132	-2.001862	0.515494	0.001932	0.714288
-9.604930	-1.973210	0.520499	0.001967	0.714278
-9.389935	-2.020998	0.525504	0.001927	0.714259
-9.828881	-2.086080	0.530509	0.002009	0.713975
-10.257901	-2.010013	0.535514	0.002089	0.713974
-10.335532	-1.993369	0.540518	0.002103	0.713980
-10.124084	-2.035219	0.545523	0.002064	0.713971
-10.280078	-2.004260	0.550528	0.002093	0.713978
-10.617576	-1.945559	0.555533	0.002155	0.713975
-10.715173	-2.058636	0.560538	0.002173	0.713716
-11.505473	-1.943954	0.565542	0.002320	0.713664
-11.626290	-1.928568	0.570547	0.002343	0.713652
-10.972966	-2.041096	0.575552	0.002221	0.713660
-11.283492	-1.986335	0.580557	0.002279	0.713659
-11.669609	-1.921600	0.585562	0.002351	0.713651
-10.989861	-2.037149	0.590566	0.002224	0.713662
-11.737929	-2.040356	0.595571	0.002363	0.713391
-12.281495	-1.955767	0.600576	0.002465	0.713366
-11.995112	-2.006649	0.605581	0.002411	0.713367
-11.700417	-2.061211	0.610586	0.002356	0.713363
-11.930119	-2.018180	0.615590	0.002399	0.713367
-12.210205	-1.972059	0.620595	0.002451	0.713360
-11.782789	-2.117637	0.625600	0.002372	0.713222
-12.704288	-2.050358	0.630605	0.002543	0.713029
-12.920492	-2.012753	0.635610	0.002583	0.713027
-12.871768	-2.016546	0.640614	0.002574	0.713037
-13.136185	-1.974822	0.645619	0.002623	0.713027
-12.915225	-2.012873	0.650624	0.002582	0.713029
-12.904281	-2.014131	0.655629	0.002580	0.713031
-13.527382	-2.036335	0.660634	0.002696	0.712766
-13.757586	-2.020071	0.665638	0.002739	0.712717
-14.091735	-1.963801	0.670643	0.002801	0.712710
-13.746675	-2.022084	0.675648	0.002737	0.712717
-13.796365	-2.011834	0.680653	0.002746	0.712719
-14.175376	-1.948668	0.685658	0.002816	0.712711
-13.736288	-2.021587	0.690662	0.002735	0.712722
-13.876752	-2.116087	0.695667	0.002761	0.712484
-15.029187	-1.955786	0.700672	0.002975	0.712394
-15.022849	-1.956616	0.705677	0.002974	0.712395
-14.488713	-2.053882	0.710682	0.002874	0.712391
-14.595705	-2.030600	0.715686	0.002894	0.712399
-14.853717	-1.990716	0.720691	0.002942	0.712387
-14.586308	-2.033167	0.725696	0.002892	0.712398
-14.888798	-2.102577	0.730701	0.002949	0.712152
-15.977892	-1.938613	0.735706	0.003151	0.712092
-15.900015	-1.949136	0.740710	0.003137	0.712099
-15.508276	-2.021421	0.745715	0.003064	0.712094
-15.654519	-1.995495	0.750720	0.003091	0.712094
-15.583478	-2.004917	0.755725	0.003078	0.712101
-15.720388	-1.985511	0.760730	0.003103	0.712091
-15.815288	-2.074822	0.765734	0.003121	0.711879
-16.735340	-1.970052	0.770739	0.003292	0.711761
-16.422541	-2.023181	0.775744	0.003234	0.711767
-16.220920	-2.058732	0.780749	0.003196	0.711768
-16.908819	-1.938753	0.785754	0.003324	0.711762
-16.486014	-2.008431	0.790758	0.003245	0.711774
-16.364196	-2.035908	0.795763	0.003223	0.711762
-16.979393	-2.034177	0.800768	0.003337	0.711547
-17.539352	-1.976871	0.805773	0.003441	0.711463
-17.451851	-1.995843	0.810778	0.003425	0.711456
-17.146732	-2.044202	0.815782	0.003368	0.711468
-17.930923	-1.909057	0.820787	0.003514	0.711459
-17.515498	-1.982863	0.825792	0.003437	0.711460
-17.299494	-2.020665	0.830797	0.003396	0.711461
-17.576771	-2.036887	0.835802	0.003448	0.711330
-18.517442	-1.960541	0.840806	0.003623	0.711148
-18.258199	-2.010859	0.845811	0.003575	0.711140
-18.376156	-1.986569	0.850816	0.003597	0.711147
-18.358649	-1.989860	0.855821	0.003593	0.711147
-18.333263	-1.997019	0.860826	0.003589	0.711142
-18.123290	-2.030930	0.865830	0.003549	0.711149
-18.367969	-2.029740	0.870835	0.003595	0.711064
-19.362744	-1.945785	0.875840	0.003780	0.710878
-18.791234	-2.047214	0.880845	0.003674	0.710879
-19.361836	-1.948987	0.885850	0.003780	0.710872
-18.942188	-2.017841	0.890854	0.003702	0.710884
-18.836050	-2.041227	0.895859	0.003682	0.710875
-19.139445	-1.986082	0.900864	0.003738	0.710877
-19.403969	-2.023242	0.905869	0.003787	0.710709
-20.208483	-1.967864	0.910874	0.003937	0.710534
-19.553812	-2.077238	0.915878	0.003815	0.710548
-20.258181	-1.956810	0.920883	0.003946	0.710538
-20.616875	-1.892005	0.925888	0.004013	0.710540
-19.774486	-2.039911	0.930893	0.003856	0.710545
-20.091688	-1.987228	0.935898	0.003915	0.710537
-20.367710	-1.998151	0.940902	0.003966	0.710417
-21.121086	-1.961063	0.945907	0.004107	0.710223
-20.687312	-2.036936	0.950912	0.004026	0.710226
-20.984826	-1.982759	0.955917	0.004081	0.710229
-21.175589	-1.951395	0.960922	0.004117	0.710223
-20.740095	-2.026637	0.965926	0.004036	0.710228
-20.881006	-2.005681	0.970931	0.004062	0.710220
-21.064600	-2.024103	0.975936	0.004096	0.710118
-21.792471	-2.005062	0.980941	0.004231	0.709897
-21.802640	-2.004358	0.985946	0.004233	0.709895
-21.964905	-1.971590	0.990950	0.004263	0.709902
-21.673940	-2.026426	0.995955	0.004209	0.709897
-21.722937	-2.016577	1.000960	0.004218	0.709899
-22.101977	-1.947168	1.005965	0.004289	0.709903
-22.343369	-1.912050	1.010970	0.004333	0.709887
-22.079304	-2.098627	1.015974	0.004284	0.709608
-22.557947	-2.017672	1.020979	0.004373	0.709600
-23.245624	-1.893921	1.025984	0.004501	0.709602
-22.671291	-1.994575	1.030989	0.004394	0.709606
-22.644325	-2.002791	1.035994	0.004389	0.709599
-22.988164	-1.937391	1.040998	0.004453	0.709607
-22.985489	-1.942254	1.046003	0.004453	0.709599
-23.046561	-2.079448	1.051008	0.004464	0.709303
-23.567054	-2.000040	1.056013	0.004561	0.709276
-23.852638	-1.953994	1.061018	0.004614	0.709266
-23.591276	-1.996143	1.066022	0.004565	0.709275
-23.870530	-1.950797	1.071027	0.004617	0.709267
-24.033816	-1.921009	1.076032	0.004647	0.709268
-23.660526	-1.985992	1.081037	0.004578	0.709271
-24.053189	-2.016838	1.086042	0.004651	0.709070
-24.955801	-1.908622	1.091046	0.004819	0.708964
-24.585046	-1.977288	1.096051	0.004750	0.708959
-24.315160	-2.023766	1.101056	0.004700	0.708963
-24.474146	-1.995914	1.106061	0.004729	0.708962
-24.778356	-1.943465	1.111066	0.004786	0.708958
-24.295413	-2.025264	1.116070	0.004696	0.708967
-24.425233	-2.090360	1.121075	0.004720	0.708790
-25.905578	-1.899532	1.126080	0.004995	0.708644
-25.606847	-1.951699	1.131085	0.004940	0.708647
-25.399818	-1.992626	1.136090	0.004901	0.708639
-25.373170	-1.994234	1.141094	0.004896	0.708645
-25.694539	-1.940401	1.146099	0.004956	0.708638
-25.529304	-1.969632	1.151104	0.004925	0.708639
-25.494806	-2.016320	1.156109	0.004919	0.708558
-26.353347	-1.967645	1.161114	0.005078	0.708349
-25.956857	-2.033108	1.166118	0.005005	0.708359
-26.309186	-1.972781	1.171123	0.005070	0.708354
-26.249065	-1.984018	1.176128	0.005059	0.708353
-26.068568	-2.013827	1.181133	0.005025	0.708358
-26.491401	-1.943699	1.186138	0.005104	0.708348
-26.199120	-2.085230	1.191142	0.005049	0.708169
-27.392996	-1.949627	1.196147	0.005272	0.708014
-27.211453	-1.982506	1.201152	0.005238	0.708013
-26.978233	-2.020157	1.206157	0.005194	0.708021
-27.649674	-1.903728	1.211162	0.005319	0.708015
-27.191863	-1.982344	1.216166	0.005234	0.708021
-27.039426	-2.011437	1.221171	0.005206	0.708017
-27.363154	-2.024485	1.226176	0.005266	0.707875
-28.246997	-1.952353	1.231181	0.005430	0.707704
-27.907884	-2.015147	1.236186	0.005367	0.707700
-27.967672	-1.999563	1.241190	0.005378	0.707710
-28.531777	-1.904052	1.246195	0.005483	0.707700
-28.459114	-1.915345	1.251200	0.005470	0.707703
-27.970824	-1.999864	1.256205	0.005379	0.707708
-28.430903	-1.925463	1.261210	0.005464	0.707693
-28.754468	-2.022568	1.266214	0.005524	0.707383
-29.068640	-1.967401	1.271219	0.005583	0.707381
-29.437440	-1.902496	1.276224	0.005651	0.707380
-28.773835	-2.018539	1.281229	0.005528	0.707384
-28.932857	-1.993516	1.286234	0.005557	0.707378
-29.131757	-1.955005	1.291238	0.005594	0.707384
-29.285867	-1.929885	1.296243	0.005623	0.707379
-29.308530	-2.034634	1.301248	0.005627	0.707161
-29.850619	-1.975427	1.306253	0.005728	0.707086
-30.115712	-1.929589	1.311258	0.005777	0.707083
-30.005648	-1.945608	1.316262	0.005757	0.707091
-30.000815	-1.949750	1.321267	0.005756	0.707084
-29.821584	-1.981557	1.326272	0.005722	0.707084
-29.884440	-1.967180	1.331277	0.005734	0.707091
-30.414430	-1.993695	1.336282	0.005833	0.706848
-30.833635	-1.963523	1.341286	0.005911	0.706759
-30.864437	-1.961584	1.346291	0.005916	0.706752
-30.833711	-1.964550	1.351296	0.005911	0.706757
-30.575350	-2.008987	1.356301	0.005862	0.706760
-30.660155	-1.997927	1.361306	0.005878	0.706752
-30.761654	-1.974953	1.366310	0.005897	0.706762
-30.985933	-2.053648	1.371315	0.005939	0.706524
-31.640439	-1.973819	1.376320	0.006060	0.706450
-31.422112	-2.011703	1.381325	0.006020	0.706452
-31.538402	-1.993087	1.386330	0.006041	0.706448
-31.345292	-2.024184	1.391334	0.006005	0.706455
-31.539707	-1.992573	1.396339	0.006042	0.706449
-31.589154	-2.010730	1.401344	0.006051	0.706395
-32.120785	-2.043618	1.406349	0.006150	0.706138
-32.575814	-1.967334	1.411354	0.006234	0.706129
-32.703697	-1.940981	1.416358	0.006258	0.706136
-32.350084	-2.006594	1.421363	0.006192	0.706131
-32.372788	-2.003299	1.426368	0.006196	0.706129
-32.763334	-1.928765	1.431373	0.006269	0.706139
-32.791089	-1.929967	1.436378	0.006274	0.706127
-32.910387	-2.036111	1.441382	0.006296	0.705871
-33.297050	-1.970419	1.446387	0.006368	0.705865
-33.740568	-1.890556	1.451392	0.006451	0.705866
-33.253066	-1.975458	1.456397	0.006360	0.705871
-33.378164	-1.955967	1.461402	0.006383	0.705865
-33.515280	-1.928201	1.466406	0.006409	0.705872
-33.354457	-1.959059	1.471411	0.006379	0.705867
-33.942899	-2.020274	1.476416	0.006488	0.705533
-34.256265	-1.964271	1.481421	0.006546	0.705534
-34.493066	-1.925253	1.486426	0.006590	0.705527
-34.203661	-1.973137	1.491430	0.006536	0.705535
-34.336585	-1.952947	1.496435	0.006561	0.705528
-34.629304	-1.900508	1.501440	0.006616	0.705529
-34.202180	-1.974067	1.506445	0.006536	0.705534
-34.830135	-1.993918	1.511450	0.006653	0.705269
-35.407137	-1.916738	1.516454	0.006760	0.705217
-35.177955	-1.959975	1.521459	0.006718	0.705213
-34.994556	-1.992840	1.526464	0.006683	0.705212
-35.156667	-1.960699	1.531469	0.006713	0.705219
-35.154899	-1.964906	1.536474	0.006713	0.705211
-34.761439	-2.032816	1.541478	0.006640	0.705216
-35.635784	-2.023638	1.546483	0.006803	0.704921
-36.307252	-1.919874	1.551488	0.006927	0.704889
-36.001783	-1.971712	1.556493	0.006871	0.704894
-35.726579	-2.025633	1.561498	0.006819	0.704884
-36.138462	-1.947802	1.566502	0.006896	0.704893
-36.233345	-1.931638	1.571507	0.006913	0.704892
-36.041442	-1.967028	1.576512	0.006878	0.704890
-36.127490	-2.064144	1.581517	0.006894	0.704663
-37.089609	-1.926646	1.586522	0.007073	0.704595
-36.873301	-1.962086	1.591526	0.007032	0.704601
-37.047533	-1.932783	1.596531	0.007065	0.704598
-37.140204	-1.916122	1.601536	0.007082	0.704598
-36.640587	-2.002420	1.606541	0.006989	0.704604
-37.001647	-1.944573	1.611546	0.007056	0.704591
-37.549865	-1.979183	1.616550	0.007158	0.704324
-37.752813	-1.974378	1.621555	0.007196	0.704261
-37.524468	-2.015065	1.626560	0.007153	0.704261
-37.570401	-2.003484	1.631565	0.007162	0.704268
-38.102031	-1.913055	1.636570	0.007261	0.704259
-37.606170	-1.998338	1.641574	0.007168	0.704266
-37.511214	-2.020509	1.646579	0.007151	0.704255
-38.839415	-1.933445	1.651584	0.007398	0.703954
-38.605666	-1.971729	1.656589	0.007354	0.703961
-38.714413	-1.957155	1.661594	0.007374	0.703951
-38.543607	-1.984488	1.666598	0.007343	0.703957
-38.590064	-1.978272	1.671603	0.007351	0.703953
-38.586970	-1.978800	1.676608	0.007351	0.703953
-38.566020	-1.980422	1.681613	0.007347	0.703958
-39.035692	-2.050725	1.686618	0.007434	0.703647
-39.562868	-1.957833	1.691622	0.007532	0.703645
-39.735907	-1.930633	1.696627	0.007564	0.703638
-39.590887	-1.958013	1.701632	0.007537	0.703635
-39.380911	-1.991133	1.706637	0.007498	0.703644
-39.779616	-1.925594	1.711642	0.007572	0.703633
-39.729255	-1.930179	1.716646	0.007563	0.703642
-39.968572	-1.997437	1.721651	0.007607	0.703420
-40.436233	-1.953704	1.726656	0.007694	0.703340
-40.373082	-1.961769	1.731661	0.007682	0.703346
-40.719621	-1.902164	1.736666	0.007747	0.703342
-40.205967	-1.990629	1.741670	0.007651	0.703349
-40.226936	-1.990076	1.746675	0.007655	0.703342
-40.755926	-1.897206	1.751680	0.007754	0.703339
-40.896692	-1.984962	1.756685	0.007780	0.703112
-41.505522	-1.931070	1.761690	0.007893	0.703001
-41.222741	-1.976404	1.766694	0.007840	0.703012
-41.327603	-1.960003	1.771699	0.007860	0.703007
-41.674077	-1.902261	1.776704	0.007924	0.702999
-41.148652	-1.991206	1.781709	0.007826	0.703009
-41.385325	-1.952231	1.786714	0.007870	0.703002
-41.481230	-2.022238	1.791718	0.007888	0.702827
-42.373309	-1.928131	1.796723	0.008054	0.702696
-42.134878	-1.972629	1.801728	0.008010	0.702692
-41.916364	-2.006160	1.806733	0.007969	0.702703
-42.308450	-1.942523	1.811738	0.008042	0.702690
-42.366470	-1.927828	1.816742	0.008053	0.702699
-42.368730	-1.930106	1.821747	0.008053	0.702694
-42.065704	-2.075645	1.826752	0.007997	0.702509
-43.005567	-1.972945	1.831757	0.008172	0.702378
-43.287343	-1.928779	1.836762	0.008224	0.702366
-43.042076	-1.969053	1.841766	0.008178	0.702373
-42.816483	-2.010413	1.846771	0.008136	0.702371
-43.024722	-1.973877	1.851776	0.008175	0.702369
-43.199113	-1.940210	1.856781	0.008207	0.702375
-43.557535	-1.980386	1.861786	0.008274	0.702164
-44.082841	-1.929573	1.866790	0.008372	0.702078
-43.861733	-1.970403	1.871795	0.008331	0.702075
-44.105852	-1.928781	1.876800	0.008376	0.702071
-44.187978	-1.909676	1.881805	0.008391	0.702081
-44.076073	-1.934121	1.886810	0.008370	0.702072
-44.083494	-1.929070	1.891814	0.008372	0.702079
-43.806107	-2.045264	1.896819	0.008320	0.701944
-45.144010	-1.906358	1.901824	0.008569	0.701743
-44.518045	-2.015022	1.906829	0.008452	0.701749
-44.779818	-1.971638	1.911834	0.008501	0.701742
-44.976014	-1.934856	1.916838	0.008537	0.701746
-44.953233	-1.938587	1.921843	0.008533	0.701747
-44.794664	-1.966337	1.926848	0.008504	0.701748
-44.386389	-2.127049	1.931853	0.008428	0.701570
-45.929010	-1.918654	1.936858	0.008715	0.701435
-45.961044	-1.909719	1.941862	0.008721	0.701442
-45.448207	-2.002262	1.946867	0.008625	0.701440
-45.767486	-1.948660	1.951872	0.008684	0.701433
-45.718052	-1.951399	1.956877	0.008675	0.701446
-45.820473	-1.939320	1.961882	0.008694	0.701433
-45.829376	-2.038357	1.966886	0.008696	0.701230
-46.786523	-1.917986	1.971891	0.008874	0.701128
-46.736913	-1.928890	1.976896	0.008865	0.701124
-46.340832	-1.997224	1.981901	0.008791	0.701129
-46.596812	-1.955831	1.986906	0.008838	0.701120
-46.535209	-1.963210	1.991910	0.008827	0.701127
-46.467326	-1.975638	1.996915	0.008814	0.701127
-47.117420	-1.965242	2.001920	0.008935	0.700913

-46.974792	-2.010417	2.011917	0.008909	0.700873
-47.468560	-1.919658	2.021914	0.009000	0.700879
-47.189979	-1.968518	2.031910	0.008948	0.700881
-47.164332	-1.974318	2.041907	0.008944	0.700879
-47.211785	-1.965655	2.051904	0.008952	0.700879
-47.320360	-1.949256	2.061901	0.008972	0.700874
-47.279635	-1.957205	2.071898	0.008965	0.700872
-47.094103	-1.988045	2.081894	0.008930	0.700877
-47.092646	-1.986947	2.091891	0.008930	0.700880
-47.184074	-1.971638	2.101888	0.008947	0.700878
-47.147318	-1.979381	2.111885	0.008940	0.700876
-47.283624	-1.956185	2.121882	0.008965	0.700874
-47.280116	-1.954759	2.131878	0.008964	0.700879
-47.010427	-1.917745	2.141875	0.008914	0.701051
-46.601456	-1.954784	2.151872	0.008837	0.701124
-46.587416	-1.958939	2.161869	0.008835	0.701121
-46.543304	-1.967994	2.171866	0.008826	0.701119
-46.494864	-1.928003	2.181862	0.008817	0.701218
-45.825463	-1.939061	2.191859	0.008693	0.701437
-45.597878	-1.978130	2.201856	0.008650	0.701440
-45.726953	-1.955917	2.211853	0.008674	0.701439
-45.724843	-1.911039	2.221850	0.008673	0.701531
-44.736688	-1.981084	2.231846	0.008489	0.701746
-44.869228	-1.957365	2.241843	0.008514	0.701746
-44.752255	-1.979103	2.251840	0.008492	0.701745
-44.539378	-1.921261	2.261837	0.008452	0.701939
-43.792518	-1.987162	2.271834	0.008313	0.702075
-43.829210	-1.979413	2.281830	0.008320	0.702078
-43.844000	-1.976691	2.291827	0.008322	0.702078
-43.354611	-1.958828	2.301824	0.008231	0.702291
-43.431194	-1.905312	2.311821	0.008245	0.702372
-43.271809	-1.934072	2.321818	0.008216	0.702371
-42.827426	-1.970891	2.331814	0.008133	0.702457
-42.358495	-1.935898	2.341811	0.008045	0.702697
-42.035496	-1.994604	2.351808	0.007985	0.702695
-42.332857	-1.941730	2.361805	0.008040	0.702695
-41.452780	-1.998920	2.371802	0.007876	0.702897
-41.553424	-1.925756	2.381798	0.007895	0.703008
-41.333656	-1.964004	2.391795	0.007854	0.703011
-41.178450	-1.981299	2.401792	0.007825	0.703032
-40.627861	-1.924102	2.411789	0.007722	0.703346
-40.448443	-1.958212	2.421786	0.007689	0.703342
-40.391635	-1.966977	2.431782	0.007678	0.703345
-40.298658	-1.903363	2.441779	0.007661	0.703507
-39.561424	-1.969660	2.451776	0.007523	0.703638
-39.976813	-1.896212	2.461773	0.007600	0.703637
-39.632040	-1.912821	2.471770	0.007536	0.703728
-38.755568	-1.958278	2.481766	0.007373	0.703952
-38.700769	-1.967613	2.491763	0.007363	0.703953
-38.846606	-1.941759	2.501760	0.007390	0.703953
-38.105415	-1.949685	2.511757	0.007251	0.704203
-37.894839	-1.959696	2.521754	0.007212	0.704259
-37.897004	-1.958100	2.531750	0.007212	0.704262
-37.763409	-1.936938	2.541747	0.007187	0.704353
-36.812303	-1.987252	2.551744	0.007010	0.704593
-37.087951	-1.938217	2.561741	0.007061	0.704593
-36.977845	-1.959041	2.571738	0.007041	0.704591
-36.657112	-1.911516	2.581734	0.006981	0.704802
-36.178043	-1.954196	2.591731	0.006892	0.704889
-36.186528	-1.953102	2.601728	0.006893	0.704888
-36.130363	-1.903967	2.611725	0.006883	0.705007
-35.397158	-1.933830	2.621722	0.006746	0.705211
-35.491759	-1.915248	2.631718	0.006763	0.705214
-35.213074	-1.963951	2.641715	0.006711	0.705216
-34.643731	-1.911014	2.651712	0.006605	0.705527
-34.486309	-1.940117	2.661709	0.006576	0.705526
-34.454232	-1.946836	2.671706	0.006570	0.705524
-34.282634	-1.882484	2.681702	0.006538	0.705715
-33.385601	-1.965881	2.691699	0.006371	0.705869
-33.751736	-1.901886	2.701696	0.006439	0.705867
-33.637249	-1.903751	2.711693	0.006417	0.705904
-32.965453	-1.913078	2.721690	0.006292	0.706127
-32.810671	-1.940233	2.731686	0.006263	0.706128
-32.606293	-1.976074	2.741683	0.006225	0.706129
-32.220610	-1.925726	2.751680	0.006153	0.706369
-31.981028	-1.931208	2.761677	0.006108	0.706444
-31.840246	-1.956528	2.771674	0.006082	0.706443
-31.864884	-1.909499	2.781670	0.006086	0.706529
-30.868964	-1.975055	2.791667	0.005901	0.706754
-30.987756	-1.954727	2.801664	0.005923	0.706753
-31.165313	-1.924391	2.811661	0.005956	0.706751
-30.610879	-1.882019	2.821658	0.005852	0.707034
-30.225328	-1.927301	2.831654	0.005781	0.707082
-30.058962	-1.955973	2.841651	0.005749	0.707084
-30.070986	-1.880784	2.851648	0.005752	0.707231
-29.358118	-1.936852	2.861645	0.005619	0.707373
-29.402377	-1.928097	2.871642	0.005627	0.707375
-29.404101	-1.908346	2.881638	0.005627	0.707414
-28.554102	-1.916799	2.891635	0.005469	0.707702
-28.343132	-1.954900	2.901632	0.005429	0.707701
-28.627606	-1.906056	2.911629	0.005482	0.707697
-27.895833	-1.926193	2.921626	0.005346	0.707919
-27.589566	-1.933413	2.931622	0.005289	0.708014
-27.379161	-1.970204	2.941619	0.005249	0.708016
-27.824965	-1.869685	2.951616	0.005332	0.708058
-26.701563	-1.923565	2.961613	0.005123	0.708352
-26.841401	-1.900037	2.971610	0.005149	0.708349
-26.678126	-1.929090	2.981606	0.005118	0.708349
-26.170335	-1.917698	2.991603	0.005024	0.708554
-25.920041	-1.918094	3.001600	0.004977	0.708642
-26.020777	-1.900326	3.011597	0.004996	0.708642
-25.810695	-1.896359	3.021594	0.004956	0.708725
-24.999643	-1.923812	3.031590	0.004805	0.708960
-24.906222	-1.941194	3.041587	0.004788	0.708959
-25.082186	-1.910643	3.051584	0.004820	0.708957
-24.348348	-1.913593	3.061581	0.004684	0.709214
-24.313424	-1.894345	3.071578	0.004677	0.709265
-23.811854	-1.984039	3.081574	0.004584	0.709264
-24.245736	-1.849836	3.091571	0.004664	0.709378
-23.108041	-1.941830	3.101568	0.004452	0.709600
-23.172650	-1.931283	3.111565	0.004464	0.709598
-23.313956	-1.907068	3.121562	0.004490	0.709597
-22.628426	-1.911248	3.131558	0.004363	0.709833
-22.364572	-1.925192	3.141555	0.004313	0.709899
-22.233500	-1.947682	3.151552	0.004289	0.709901
-22.231080	-1.910926	3.161549	0.004288	0.709976
-21.614098	-1.898910	3.171546	0.004173	0.710220
-21.180577	-1.976354	3.181542	0.004093	0.710220
-21.487496	-1.920710	3.191539	0.004150	0.710222
-20.778406	-1.937425	3.201536	0.004017	0.710441
-20.518119	-1.938416	3.211533	0.003969	0.710532
-20.535720	-1.935270	3.221530	0.003972	0.710532
-20.458363	-1.937659	3.231526	0.003957	0.710555
-19.696865	-1.913787	3.241523	0.003816	0.710874
-19.372926	-1.972835	3.251520	0.003755	0.710872
-19.544259	-1.940923	3.261517	0.003787	0.710875
-19.596416	-1.887772	3.271514	0.003796	0.710962
-18.642844	-1.968253	3.281510	0.003619	0.711141
-18.774844	-1.944134	3.291507	0.003643	0.711142
-18.863591	-1.928545	3.301504	0.003660	0.711142
-18.079381	-1.919076	3.311501	0.003514	0.711440
-17.916070	-1.940331	3.321498	0.003483	0.711456
-17.863379	-1.948614	3.331494	0.003473	0.711458
-17.916154	-1.857616	3.341491	0.003483	0.711621
-17.004521	-1.948052	3.351488	0.003313	0.711765
-17.273855	-1.901029	3.361485	0.003363	0.711763
-17.101407	-1.899173	3.371482	0.003331	0.711829
-16.085069	-1.947616	3.381478	0.003141	0.712093
-16.047188	-1.954552	3.391475	0.003134	0.712093
-16.301324	-1.908474	3.401472	0.003181	0.712095
-15.871816	-1.878230	3.411469	0.003101	0.712308
-15.545126	-1.897042	3.421466	0.003040	0.712386
-15.115109	-1.972163	3.431462	0.002960	0.712390
-15.337314	-1.885946	3.441459	0.003002	0.712483
-14.193106	-1.973642	3.451456	0.002788	0.712714
-14.547375	-1.911726	3.461453	0.002854	0.712712
-14.392767	-1.940166	3.471450	0.002825	0.712711
-13.704882	-1.953188	3.481446	0.002697	0.712929
-13.589829	-1.924278	3.491443	0.002676	0.713027
-13.437317	-1.951049	3.501440	0.002647	0.713028
-13.579186	-1.909935	3.511437	0.002673	0.713060
-12.711078	-1.912420	3.521434	0.002512	0.713363
-12.609979	-1.930776	3.531430	0.002493	0.713363
-12.769040	-1.902033	3.541427	0.002522	0.713364
-12.123819	-1.921885	3.551424	0.002402	0.713553
-11.783649	-1.932487	3.561421	0.002338	0.713653
-11.513027	-1.980025	3.571418	0.002288	0.713654
-11.600693	-1.963688	3.581414	0.002304	0.713656
-10.467546	-2.021078	3.591411	0.002093	0.713943
-10.674134	-1.968688	3.601408	0.002131	0.713974
-10.522622	-1.996459	3.611405	0.002103	0.713973
-10.543272	-1.993320	3.621402	0.002107	0.713972
-9.851692	-1.981450	3.631398	0.001978	0.714241
-9.644366	-1.997879	3.641395	0.001939	0.714282
-9.521206	-2.018119	3.651392	0.001916	0.714285
-9.606403	-2.003323	3.661389	0.001932	0.714285
-8.770655	-1.988653	3.671386	0.001776	0.714610
-8.922261	-1.959351	3.681382	0.001804	0.714615
-8.438252	-2.046789	3.691379	0.001714	0.714612
-8.794895	-1.946553	3.701376	0.001780	0.714686
-7.804637	-2.010902	3.711373	0.001596	0.714908
-7.840556	-2.004453	3.721370	0.001603	0.714909
-7.978580	-1.978869	3.731366	0.001628	0.714911
-7.160940	-2.014514	3.741363	0.001476	0.715129
-7.006394	-1.988023	3.751360	0.001447	0.715237
-7.032062	-1.985017	3.761357	0.001452	0.715234
-6.862872	-2.009867	3.771354	0.001420	0.715244
-5.985888	-2.013734	3.781350	0.001257	0.715547
-5.580864	-2.084220	3.791347	0.001181	0.715550
-6.069705	-1.994958	3.801344	0.001272	0.715555
-5.802477	-2.030411	3.811341	0.001222	0.715579
-5.106816	-1.998033	3.821338	0.001092	0.715889
-5.032447	-2.013164	3.831334	0.001078	0.715886
-4.908128	-2.034747	3.841331	0.001055	0.715887
-4.960489	-1.967038	3.851328	0.001065	0.716003
-4.197901	-2.037232	3.861325	0.000923	0.716133
-4.128467	-2.049866	3.871322	0.000910	0.716133
-4.384692	-2.003305	3.881318	0.000957	0.716135
-3.237661	-2.047410	3.891315	0.000744	0.716452
-3.376098	-2.023489	3.901312	0.000769	0.716451
-3.321068	-2.034228	3.911309	0.000759	0.716449
-3.306008	-1.973349	3.921306	0.000756	0.716576
-2.314808	-2.057433	3.931302	0.000571	0.716759
-2.524196	-2.019571	3.941299	0.000610	0.716760
-2.418728	-2.039335	3.951296	0.000590	0.716758
-1.944629	-1.971398	3.961293	0.000502	0.717060
-1.612530	-2.016518	3.971290	0.000440	0.717088
-1.640296	-2.012035	3.981286	0.000445	0.717087
-1.627854	-1.935259	3.991283	0.000443	0.717244
-1.486961	-1.890159	4.001280	0.000416	0.717383
-1.408917	-1.905037	4.011277	0.000402	0.717381
-1.259391	-1.802951	4.021274	0.000374	0.717636
-1.160040	-1.784537	4.031270	0.000355	0.717707
-1.040350	-1.755980	4.041267	0.000333	0.717806
-0.822424	-1.685066	4.051264	0.000292	0.718023
-0.683308	-1.703306	4.061261	0.000266	0.718036
-0.628621	-1.552903	4.071258	0.000255	0.718353
-0.683479	-1.541222	4.081254	0.000266	0.718357
-0.505143	-1.426429	4.091251	0.000232	0.718646
-0.910582	-1.321819	4.101248	0.000307	0.718711
-0.777882	-1.219583	4.111245	0.000283	0.718959
-0.487962	-1.178863	4.121242	0.000228	0.719142
-0.651764	-1.075185	4.131238	0.000259	0.719289
-0.537080	-0.936296	4.141235	0.000237	0.719603
-0.461165	-0.856704	4.151232	0.000223	0.719787
-0.594508	-0.734626	4.161229	0.000248	0.719981
-0.563818	-0.616576	4.171226	0.000242	0.720224
-0.638913	-0.446620	4.181222	0.000255	0.720533
-0.498578	-0.335175	4.191219	0.000229	0.720802
-0.352268	-0.246988	4.201216	0.000202	0.721027
-0.183997	-0.155682	4.211213	0.000170	0.721265
-0.217962	-0.010752	4.221210	0.000176	0.721539
-0.063211	0.104882	4.231206	0.000147	0.721820
0.000000	0.272252	4.241203	0.000135	0.722171

0.093179	0.870059	4.246208	0.000117	0.723377
0.310349	2.092880	4.251213	0.000076	0.725847
0.466282	3.926110	4.256218	0.000046	0.729475
0.581028	6.308408	4.261222	0.000023	0.734132
0.935611	9.164968	4.266227	-0.000045	0.739751
1.314578	12.498737	4.271232	-0.000118	0.746245
1.747730	16.273807	4.276237	-0.000201	0.753531
2.019158	20.486415	4.281242	-0.000254	0.761509
2.424231	25.065778	4.286246	-0.000333	0.770124
3.033196	29.989181	4.291251	-0.000449	0.779335
3.333299	35.312177	4.296256	-0.000509	0.789059
3.713199	40.933752	4.301261	-0.000583	0.799219
4.214204	46.845329	4.306266	-0.000680	0.809798
5.290662	52.930838	4.311270	-0.000885	0.820716
5.894881	59.393567	4.316275	-0.001002	0.831991
6.815383	66.016388	4.321280	-0.001178	0.843478
7.327174	72.941648	4.326285	-0.001277	0.855193
8.149141	80.018116	4.331290	-0.001435	0.867085
9.081119	87.265584	4.336294	-0.001613	0.879123
9.746118	94.741775	4.341299	-0.001742	0.891288
10.650542	102.334587	4.346304	-0.001916	0.903537
11.437439	110.101653	4.351309	-0.002067	0.915860
12.306710	117.969758	4.356314	-0.002234	0.928195
13.264611	125.945278	4.361318	-0.002418	0.940553
13.854757	134.103082	4.366323	-0.002533	0.952926
14.635609	142.301162	4.371328	-0.002684	0.965248
15.500702	150.578076	4.376333	-0.002850	0.977550
15.984435	159.008787	4.381338	-0.002946	0.989824
16.585219	167.446545	4.386342	-0.003063	1.001985
17.244754	175.923576	4.391347	-0.003192	1.014070
17.999131	184.407734	4.396352	-0.003338	1.026045
18.946692	192.901127	4.401357	-0.003520	1.037939
19.603995	201.478565	4.406362	-0.003648	1.049744
20.353152	210.061153	4.411366	-0.003793	1.061445
20.852871	218.723995	4.416371	-0.003892	1.073067
21.522242	227.341711	4.421376	-0.004022	1.084544
22.076728	235.998447	4.426381	-0.004131	1.095925
22.941805	244.607335	4.431386	-0.004298	1.107195
23.836325	253.217466	4.436390	-0.004470	1.118360
24.796034	261.817794	4.441395	-0.004654	1.129416
25.227766	270.503922	4.446400	-0.004741	1.140358
25.774337	279.190451	4.451405	-0.004848	1.151220
26.669536	287.789768	4.456410	-0.005020	1.161947
27.558797	296.367199	4.461414	-0.005192	1.172548
28.147005	305.004583	4.466419	-0.005307	1.183064
29.059027	313.578643	4.471424	-0.005482	1.193477
29.983741	322.123959	4.476429	-0.005660	1.203768
30.568360	330.736287	4.481434	-0.005775	1.213982
30.985062	339.346165	4.486438	-0.005858	1.224075
31.639610	347.930482	4.491443	-0.005985	1.234102
32.425168	356.436683	4.496448	-0.006137	1.243984
32.962759	364.994135	4.501453	-0.006243	1.253798
33.365188	373.552088	4.506458	-0.006324	1.263511
33.974115	382.061593	4.511462	-0.006443	1.273135
34.380292	390.580736	4.516467	-0.006524	1.282659
34.962751	399.069206	4.521472	-0.006638	1.292111
35.374711	407.557383	4.526477	-0.006720	1.301463
35.854715	416.108523	4.531482	-0.006815	1.310828
36.133693	424.637835	4.536486	-0.006873	1.320067
36.705929	433.033294	4.541491	-0.006985	1.329152
37.204651	441.445950	4.546496	-0.007083	1.338179
37.750933	449.818086	4.551501	-0.007190	1.347112
38.463737	458.193735	4.556506	-0.007329	1.356018
38.894860	466.570069	4.561510	-0.007414	1.364818
39.391515	474.963245	4.566515	-0.007512	1.373590
39.875630	483.330639	4.571520	-0.007608	1.382277
40.521896	491.682747	4.576525	-0.007734	1.390922
41.146570	500.033790	4.581530	-0.007856	1.399509
41.517435	508.386411	4.586534	-0.007930	1.408002
42.251623	516.715013	4.591539	-0.008072	1.416480
42.638569	525.054233	4.596544	-0.008150	1.424861
43.290559	533.369135	4.601549	-0.008277	1.433212
43.724857	541.700171	4.606554	-0.008363	1.441495
44.288515	549.989199	4.611558	-0.008474	1.449710
44.884996	558.300785	4.616563	-0.008590	1.457905
45.384234	566.585710	4.621568	-0.008689	1.466014
45.655579	574.977537	4.626573	-0.008745	1.474144
46.226079	583.236160	4.631578	-0.008856	1.482150
46.842874	591.477681	4.636582	-0.008977	1.490103
47.242106	599.780350	4.641587	-0.009056	1.498037
47.631885	608.053676	4.646592	-0.009134	1.505901
47.733480	616.388610	4.651597	-0.009159	1.513737
48.235749	624.628945	4.656602	-0.009258	1.521506
48.616656	632.880267	4.661606	-0.009334	1.529227
49.154891	641.126434	4.666611	-0.009440	1.536928
49.519636	649.384453	4.671616	-0.009513	1.544575
49.910466	657.643938	4.676621	-0.009591	1.552189
50.391215	665.873423	4.681626	-0.009686	1.559753
50.918331	674.070370	4.686630	-0.009790	1.567256
51.425791	682.300397	4.691635	-0.009890	1.574751
52.019381	690.501486	4.696640	-0.010006	1.582197
52.291046	698.745622	4.701645	-0.010062	1.589600
52.756564	706.986127	4.706650	-0.010154	1.596992
53.066795	715.205490	4.711654	-0.010217	1.604310
53.655625	723.409755	4.716659	-0.010332	1.611621
53.885295	731.663688	4.721664	-0.010380	1.618891
54.197442	739.874462	4.726669	-0.010444	1.626103
54.721608	748.128347	4.731674	-0.010547	1.633349
54.942835	756.324686	4.736678	-0.010593	1.640472
55.171765	764.535562	4.741683	-0.010641	1.647578
55.566385	772.731187	4.746688	-0.010720	1.654662
55.865651	780.904688	4.751693	-0.010781	1.661684
56.220141	789.100504	4.756698	-0.010853	1.668703
56.583921	797.278625	4.761702	-0.010926	1.675679
57.105621	805.423032	4.766707	-0.011028	1.682619
57.405650	813.619041	4.771712	-0.011090	1.689543
57.991587	821.772444	4.776717	-0.011204	1.696442
58.370472	829.963084	4.781722	-0.011280	1.703316
58.775648	838.130138	4.786726	-0.011361	1.710146
59.075659	846.342508	4.791731	-0.011422	1.716972
59.697700	854.451973	4.796736	-0.011543	1.723729
60.117620	862.620710	4.801741	-0.011627	1.730481
60.409215	870.822606	4.806746	-0.011687	1.737218
60.735788	878.973346	4.811750	-0.011753	1.743891
61.309572	887.116228	4.816755	-0.011865	1.750564
61.660130	895.305137	4.821760	-0.011936	1.757221
61.878060	903.465685	4.826765	-0.011982	1.763812
62.372946	911.616778	4.831770	-0.012079	1.770406
62.469948	919.821144	4.836774	-0.012103	1.776969
62.863190	927.959395	4.841779	-0.012181	1.783491
63.322635	936.108895	4.846784	-0.012272	1.790006
63.790523	944.276959	4.851789	-0.012365	1.796514
64.277356	952.395273	4.856794	-0.012461	1.802961
64.530469	960.544980	4.861798	-0.012513	1.809381
65.104108	968.675000	4.866803	-0.012625	1.815801
65.358448	976.827781	4.871808	-0.012678	1.822178
65.502513	984.997356	4.876813	-0.012710	1.828533
66.105033	993.126395	4.881818	-0.012828	1.834889
66.265728	1001.267666	4.886822	-0.012863	1.841180
66.480051	1009.431378	4.891827	-0.012908	1.847473
66.653579	1017.607539	4.896832	-0.012946	1.853749
67.105313	1025.699499	4.901837	-0.013035	1.859972
67.602648	1033.828283	4.906842	-0.013133	1.866208
67.723639	1042.007103	4.911846	-0.013161	1.872417
68.300307	1050.104791	4.916851	-0.013274	1.878596
68.623650	1058.209668	4.921856	-0.013340	1.884732
68.586689	1066.389191	4.926861	-0.013338	1.890863
69.189598	1074.476525	4.931866	-0.013456	1.896977
69.401657	1082.602172	4.936870	-0.013501	1.903056
69.852797	1090.716112	4.941875	-0.013590	1.909134
70.221063	1098.839942	4.946880	-0.013664	1.915190
70.516296	1106.942830	4.951885	-0.013724	1.921204
71.203448	1115.023934	4.956890	-0.013857	1.927226
71.323112	1123.188750	4.961894	-0.013885	1.933228
71.471301	1131.338427	4.966899	-0.013918	1.939203
71.801176	1139.444905	4.971904	-0.013985	1.945149
72.003416	1147.608129	4.976909	-0.014028	1.951103
72.443514	1155.731267	4.981914	-0.014115	1.957036
72.796611	1163.797463	4.986918	-0.014186	1.962901
73.103444	1171.905658	4.991923	-0.014249	1.968773
73.496410	1180.023738	4.996928	-0.014327	1.974644
73.834769	1188.105030	5.001933	-0.014395	1.980465
74.160535	1196.217536	5.006938	-0.014461	1.986290
74.542388	1204.325598	5.011942	-0.014538	1.992101
75.056907	1212.415716	5.016947	-0.014639	1.997896
75.614271	1220.480330	5.021952	-0.014748	2.003660
75.899266	1228.585510	5.026957	-0.014807	2.009408
76.296335	1236.726905	5.031962	-0.014886	2.015176
76.500343	1244.832249	5.036966	-0.014929	2.020883
76.941616	1252.920988	5.041971	-0.015017	2.026587
77.281349	1261.068250	5.046976	-0.015085	2.032304
77.564566	1269.181892	5.051981	-0.015143	2.037977
77.646694	1277.303769	5.056986	-0.015164	2.043618
77.860419	1285.400838	5.061990	-0.015209	2.049241
78.196156	1293.506984	5.066995	-0.015277	2.054866
78.760578	1301.559211	5.072000	-0.015387	2.060462
79.300383	1309.616203	5.077005	-0.015493	2.066044
79.961116	1317.709533	5.082010	-0.015622	2.071647
80.246288	1325.827605	5.087014	-0.015680	2.077215
80.545892	1333.915064	5.092019	-0.015741	2.082748
81.017918	1342.002900	5.097024	-0.015834	2.088283
81.406196	1350.103728	5.102029	-0.015912	2.093805
81.767974	1358.209959	5.107034	-0.015985	2.099313
82.004948	1366.303848	5.112038	-0.016034	2.104785
82.195967	1374.445201	5.117043	-0.016075	2.110271
82.462921	1382.607440	5.122048	-0.016130	2.115764
82.740162	1390.646684	5.127053	-0.016187	2.121162
83.048956	1398.722729	5.132058	-0.016250	2.126573
83.366717	1406.805844	5.137062	-0.016314	2.131977
83.753218	1414.886413	5.142067	-0.016392	2.137371
84.131168	1422.953007	5.147072	-0.016467	2.142741
84.271057	1431.063811	5.152077	-0.016499	2.148105
84.918880	1439.131385	5.157082	-0.016625	2.153474
85.411163	1447.178236	5.162086	-0.016722	2.158802
85.592063	1455.286183	5.167091	-0.016761	2.164128
85.975860	1463.371952	5.172096	-0.016837	2.169444
86.159039	1471.491041	5.177101	-0.016877	2.174751
86.502068	1479.578070	5.182106	-0.016946	2.180039
86.874720	1487.644643	5.187110	-0.017021	2.185303
86.976103	1495.772524	5.192115	-0.017045	2.190570
87.436499	1503.841172	5.197120	-0.017136	2.195818
87.731315	1511.892895	5.202125	-0.017196	2.201028
88.031728	1519.977250	5.207130	-0.017258	2.206246
88.120666	1528.086865	5.212134	-0.017279	2.211450
88.488157	1536.166448	5.217139	-0.017353	2.216647
88.850242	1544.228043	5.222144	-0.017426	2.221820
89.117071	1552.289389	5.227149	-0.017481	2.226972
89.368378	1560.414137	5.232154	-0.017533	2.232151
89.674623	1568.475481	5.237158	-0.017595	2.237282
90.147397	1576.519935	5.242163	-0.017689	2.242406
90.580099	1584.591207	5.247168	-0.017775	2.247532
91.248935	1592.624476	5.252173	-0.017904	2.252642
91.795390	1600.721895	5.257178	-0.018012	2.257770
91.974809	1608.807476	5.262182	-0.018050	2.262847
92.164511	1616.915184	5.267187	-0.018091	2.267928
92.629951	1625.056692	5.272192	-0.018183	2.273042
92.782617	1633.126430	5.277197	-0.018217	2.278072
93.121074	1641.172595	5.282202	-0.018285	2.283093
93.240604	1649.235362	5.287206	-0.018313	2.288095
93.555138	1657.314307	5.292211	-0.018376	2.293112
93.857110	1665.376141	5.297216	-0.018438	2.298106
94.010795	1673.431886	5.302221	-0.018472	2.303074
94.400974	1681.509632	5.307226	-0.018550	2.308063
94.707247	1689.583200	5.312230	-0.018612	2.313033
94.968631	1697.649036	5.317235	-0.018666	2.317983
95.509532	1705.677219	5.322240	-0.018772	2.322923
95.480977	1713.781006	5.327245	-0.018772	2.327851
95.738757	1721.873522	5.332250	-0.018826	2.332786
96.026779	1729.935143	5.337254	-0.018884	2.337693
96.411132	1737.980414	5.342259	-0.018961	2.342589
96.778710	1746.046356	5.347264	-0.019035	2.347485
96.880243	1754.166973	5.352269	-0.019059	2.352382
97.265085	1762.212453	5.357274	-0.019136	2.357247
97.374251	1770.287277	5.362278	-0.019162	2.362097
97.510639	1778.337243	5.367283	-0.019193	2.366925
97.702170	1786.450234	5.372288	-0.019234	2.371784
97.896868	1794.493040	5.377293	-0.019275	2.376592
98.272874	1802.548174	5.382298	-0.019351	2.381412
98.452908	1810.611659	5.387302	-0.019389	2.386212
98.877839	1818.648184	5.392307	-0.019474	2.391005
99.172183	1826.741313	5.397312	-0.019534	2.395812
99.379608	1834.783559	5.402317	-0.019578	2.400572
100.021085	1842.796828	5.407322	-0.019703	2.405340
100.153340	1850.889916	5.412326	-0.019733	2.410105
100.449591	1858.973338	5.417331	-0.019793	2.414868
100.917434	1867.013851	5.422336	-0.019885	2.419610
100.981720	1875.080027	5.427341	-0.019903	2.424326
101.252050	1883.183230	5.432346	-0.019958	2.429070
101.487602	1891.322097	5.437350	-0.020008	2.433823
101.869203	1899.330226	5.442355	-0.020084	2.438503
102.185171	1907.364251	5.447360	-0.020148	2.443183
102.505310	1915.392817	5.452365	-0.020213	2.447851
102.948644	1923.463516	5.457370	-0.020301	2.452544
102.989979	1931.552495	5.462374	-0.020314	2.457208
103.258758	1939.595595	5.467379	-0.020369	2.461853
103.582969	1947.643560	5.472384	-0.020435	2.466497
104.064522	1955.679834	5.477389	-0.020530	2.471138
104.331244	1963.777281	5.482394	-0.020585	2.475788
104.468284	1971.816943	5.487398	-0.020616	2.480387
104.953900	1979.846911	5.492403	-0.020711	2.484998
105.258025	1987.909606	5.497408	-0.020773	2.489605
105.725176	1995.966325	5.502413	-0.020866	2.494212
106.079367	2004.026655	5.507418	-0.020937	2.498805
106.083535	2012.107455	5.512422	-0.020943	2.503375
106.266672	2020.178576	5.517427	-0.020982	2.507944
106.620523	2028.270574	5.522432	-0.021054	2.512529
106.806181	2036.326972	5.527437	-0.021093	2.517073
107.084600	2044.359154	5.532442	-0.021151	2.521603
107.194120	2052.417008	5.537446	-0.021176	2.526126
107.653042	2060.437137	5.542451	-0.021267	2.530645
108.045143	2068.508414	5.547456	-0.021345	2.535180
108.230820	2076.538593	5.552461	-0.021385	2.539669
108.442532	2084.606465	5.557466	-0.021430	2.544173
108.848459	2092.655074	5.562470	-0.021511	2.548671
109.095101	2100.727962	5.567475	-0.021562	2.553164
109.275103	2108.794884	5.572480	-0.021601	2.557641
109.509816	2116.828978	5.577485	-0.021650	2.562096
109.660223	2124.900612	5.582490	-0.021683	2.566558
109.873794	2132.961111	5.587494	-0.021728	2.571011
110.264311	2141.002058	5.592499	-0.021806	2.575457
110.733232	2149.048994	5.597504	-0.021899	2.579904
110.817429	2157.089110	5.602509	-0.021920	2.584313
111.189966	2165.150865	5.607514	-0.021995	2.588747
111.537179	2173.356083	5.612518	-0.022065	2.593249
111.591464	2181.431750	5.617523	-0.022080	2.597652
112.046600	2189.397599	5.622528	-0.022170	2.602016
112.415006	2197.386184	5.627533	-0.022244	2.606379
112.711469	2205.442583	5.632538	-0.022304	2.610766
112.654127	2213.528094	5.637542	-0.022299	2.615138
112.993896	2221.513660	5.642547	-0.022368	2.619476
113.465698	2229.545850	5.647552	-0.022461	2.623839
113.736435	2237.594514	5.652557	-0.022516	2.628192
114.137373	2245.652241	5.657562	-0.022596	2.632550
114.355948	2253.709077	5.662566	-0.022642	2.636888
114.763695	2261.733590	5.667571	-0.022724	2.641215
115.260426	2269.784235	5.672576	-0.022821	2.645554
115.400527	2277.825157	5.677581	-0.022853	2.649857
115.793022	2285.914845	5.682586	-0.022931	2.654196
116.107670	2293.947992	5.687590	-0.022995	2.658493
116.290305	2301.992219	5.692595	-0.023034	2.662779
116.581001	2310.064621	5.697600	-0.023094	2.667081
116.522683	2318.152008	5.702605	-0.023088	2.671362
116.844292	2326.232177	5.707610	-0.023154	2.675656
117.226714	2334.216958	5.712614	-0.023230	2.679896
117.410271	2342.252333	5.717619	-0.023269	2.684144
117.350780	2350.338250	5.722624	-0.023264	2.688396
117.618420	2358.362374	5.727629	-0.023319	2.692630
118.149453	2366.391962	5.732634	-0.023423	2.696876
118.322717	2374.426278	5.737638	-0.023461	2.701096
118.525259	2382.453022	5.742643	-0.023504	2.705307
118.949617	2390.503488	5.747648	-0.023588	2.709538
119.258281	2398.562067	5.752653	-0.023651	2.713759
119.531155	2406.610650	5.757658	-0.023707	2.717966
119.779511	2414.627907	5.762662	-0.023758	2.722148
119.914655	2422.674145	5.767667	-0.023789	2.726332
120.174762	2430.758363	5.772672	-0.023842	2.730537
120.368714	2438.799045	5.777677	-0.023884	2.734709
120.582748	2446.858211	5.782682	-0.023929	2.738885
120.860347	2454.885333	5.787686	-0.023986	2.743043
121.078595	2462.930600	5.792691	-0.024032	2.747199
121.192761	2471.053325	5.797696	-0.024059	2.751383
121.452809	2479.139662	5.802701	-0.024112	2.755551
121.591375	2487.139936	5.807706	-0.024143	2.759661
121.896387	2495.149161	5.812710	-0.024205	2.763779
122.222167	2503.164412	5.817715	-0.024271	2.767895
122.470076	2511.238240	5.822720	-0.024323	2.772031
122.741482	2519.268190	5.827725	-0.024379	2.776139
123.090034	2527.285235	5.832730	-0.024449	2.780239
123.381675	2535.304957	5.837734	-0.024508	2.784331
123.569650	2543.369019	5.842739	-0.024549	2.788433
123.987338	2551.409166	5.847744	-0.024632	2.792531
124.139774	2559.458737	5.852749	-0.024666	2.796612
124.499903	2567.488101	5.857754	-0.024738	2.800688
124.752883	2575.505195	5.862758	-0.024790	2.804747
124.951003	2583.571391	5.867763	-0.024832	2.808821
125.221923	2591.627993	5.872768	-0.024888	2.812888
125.210470	2599.697741	5.877773	-0.024891	2.816940
125.562541	2607.731195	5.882778	-0.024962	2.820988
125.755154	2615.750347	5.887782	-0.025003	2.825015
125.950860	2623.813817	5.892787	-0.025045	2.829058
126.210101	2631.902339	5.897792	-0.025099	2.833111
126.243180	2639.928719	5.902797	-0.025110	2.837115
126.541481	2647.939447	5.907802	-0.025171	2.841120
126.855936	2655.945364	5.912806	-0.025235	2.845118
127.368855	2663.962892	5.917811	-0.025336	2.849127
127.497899	2672.078904	5.922816	-0.025365	2.853158
127.660125	2680.074617	5.927821	-0.025400	2.857125
128.150319	2688.114090	5.932826	-0.025497	2.861127
128.295954	2696.141845	5.937830	-0.025529	2.865098
128.344555	2704.213270	5.942835	-0.025544	2.869080
128.749197	2712.271887	5.947840	-0.025624	2.873070
129.120428	2720.287844	5.952845	-0.025699	2.877031
129.262753	2728.340635	5.957850	-0.025731	2.880992
129.279936	2736.368848	5.962854	-0.025739	2.884929
129.765120	2744.384011	5.967859	-0.025835	2.888880
130.008199	2752.453302	5.972864	-0.025885	2.892838
130.048659	2760.507637	5.977869	-0.025898	2.896773
130.342895	2768.553173	5.982874	-0.025958	2.900711
130.539094	2776.569321	5.987878	-0.026000	2.904625
130.984398	2784.582393	5.992883	-0.026088	2.908545
131.319550	2792.708088	5.997888	-0.026156	2.912509
131.653056	2800.757606	6.002893	-0.026223	2.916430
131.714881	2808.778299	6.007898	-0.026240	2.920318
131.915020	2816.761618	6.012902	-0.026283	2.924189
132.119426	2824.790740	6.017907	-0.026326	2.928078
132.430349	2832.859179	6.022912	-0.026389	2.931986
132.423398	2840.907703	6.027917	-0.026393	2.935863
132.749500	2848.894261	6.032922	-0.026459	2.939722
133.006660	2856.941251	6.037926	-0.026513	2.943601
133.088999	2864.969121	6.042931	-0.026533	2.947457
133.422490	2873.041661	6.047936	-0.026601	2.951343
133.508038	2881.088483	6.052941	-0.026622	2.955198
133.881089	2889.101134	6.057946	-0.026697	2.959046
134.088746	2897.125861	6.062950	-0.026740	2.962887
134.515424	2905.146106	6.067955	-0.026825	2.966732
134.947332	2913.191522	6.072960	-0.026911	2.970584
134.691498	2921.277216	6.077965	-0.026869	2.974415
134.873863	2929.323749	6.082970	-0.026908	2.978244
135.344496	2937.315737	6.087974	-0.027001	2.982058
135.298984	2945.363269	6.092979	-0.026998	2.985867
135.710051	2953.397637	6.097984	-0.027079	2.989687
135.815016	2961.454476	6.102989	-0.027104	2.993499
135.983642	2969.511593	6.107994	-0.027141	2.997308
136.069365	2977.534775	6.112998	-0.027162	3.001092
136.450122	2985.501162	6.118003	-0.027238	3.004860
136.713216	2993.559274	6.123008	-0.027293	3.008660
136.933055	3001.602981	6.128013	-0.027339	3.012447
137.238430	3009.669282	6.133018	-0.027401	3.016243
137.703122	3017.655832	6.138022	-0.027493	3.020005
137.905232	3025.686049	6.143027	-0.027536	3.023770
138.179796	3033.745584	6.148032	-0.027592	3.027547
138.342232	3041.786155	6.153037	-0.027628	3.031305
138.802796	3049.829282	6.158042	-0.027719	3.035075
138.929006	3057.864298	6.163046	-0.027748	3.038819
139.032233	3065.882769	6.168051	-0.027772	3.042550
139.440820	3073.929393	6.173056	-0.027854	3.046304
139.490582	3081.976002	6.178061	-0.027868	3.050037
139.832778	3090.038829	6.183066	-0.027937	3.053786
140.111418	3098.052748	6.188070	-0.027994	3.057505
140.221778	3106.087749	6.193075	-0.028020	3.061221
140.359793	3114.103334	6.198080	-0.028051	3.064925
140.616697	3122.133496	6.203085	-0.028104	3.068637
140.823747	3130.230878	6.208090	-0.028148	3.072372
141.183953	3138.309047	6.213094	-0.028220	3.076102
141.489244	3146.268726	6.218099	-0.028283	3.079770
141.728519	3154.294490	6.223104	-0.028332	3.083461
141.813641	3162.301941	6.228109	-0.028354	3.087132
141.927686	3170.365910	6.233114	-0.028380	3.090825
142.205168	3178.414909	6.238118	-0.028437	3.094515
142.404809	3186.402080	6.243123	-0.028479	3.098169
142.637034	3194.451036	6.248128	-0.028528	3.101848
142.883818	3202.442334	6.253133	-0.028579	3.105497
143.210905	3210.495591	6.258138	-0.028645	3.109173
143.283570	3218.574326	6.263142	-0.028664	3.112846
143.260483	3226.618469	6.268147	-0.028665	3.116493
143.759526	3234.595972	6.273152	-0.028763	3.120130
143.976638	3242.610337	6.278157	-0.028809	3.123767
143.904208	3250.687719	6.283162	-0.028801	3.127414
144.216705	3258.717765	6.288166	-0.028864	3.131054
144.340219	3266.744793	6.293171	-0.028893	3.134679
144.930921	3274.762223	6.298176	-0.029008	3.138316
144.975521	3282.797800	6.303181	-0.029022	3.141934
145.317977	3290.823878	6.308186	-0.029091	3.145555
145.482812	3298.878862	6.313190	-0.029127	3.149178
145.582825	3306.950938	6.318195	-0.029151	3.152802
145.860904	3315.009415	6.323200	-0.029208	3.156422
146.170051	3322.948565	6.328205	-0.029271	3.159987
146.363884	3330.993336	6.333210	-0.029312	3.163590
146.622236	3339.010330	6.338214	-0.029365	3.167179
146.798860	3347.054270	6.343219	-0.029403	3.170772
146.819496	3355.128802	6.348224	-0.029413	3.174369
146.960974	3363.146786	6.353229	-0.029444	3.177941
147.317824	3371.162305	6.358234	-0.029516	3.181517
147.388385	3379.209568	6.363238	-0.029534	3.185091
147.518156	3387.215140	6.368243	-0.029564	3.188645
147.906782	3395.287526	6.373248	-0.029642	3.192236
148.131823	3403.315583	6.378253	-0.029689	3.195796
148.397113	3411.285241	6.383258	-0.029743	3.199328
148.610604	3419.331057	6.388262	-0.029788	3.202887
148.698375	3427.360291	6.393267	-0.029810	3.206430
149.039657	3435.388668	6.398272	-0.029879	3.209979
149.272693	3443.456921	6.403277	-0.029928	3.213537
149.706591	3451.457726	6.408282	-0.030014	3.217070
149.847362	3459.501505	6.413286	-0.030045	3.220606
149.972022	3467.507966	6.418291	-0.030074	3.224121
150.247736	3475.568305	6.423296	-0.030130	3.227661
150.420020	3483.609447	6.428301	-0.030168	3.231185
150.675312	3491.681037	6.433306	-0.030221	3.234722
150.873564	3499.675999	6.438310	-0.030263	3.238220
151.074715	3507.680872	6.443315	-0.030305	3.241717
151.061429	3515.712926	6.448320	-0.030308	3.245215
151.350874	3523.701247	6.453325	-0.030367	3.248701
151.603711	3531.770684	6.458330	-0.030420	3.252218
151.935792	3539.838095	6.463334	-0.030487	3.255733
151.915294	3547.823588	6.468339	-0.030488	3.259195
152.550991	3555.837475	6.473344	-0.030612	3.262691
152.894498	3563.851624	6.478349	-0.030681	3.266172
153.037557	3571.881949	6.483354	-0.030713	3.269648
153.395966	3579.953380	6.488358	-0.030785	3.273147
153.434853	3587.993133	6.493363	-0.030798	3.276616
153.766737	3596.004712	6.498368	-0.030865	3.280081
153.737982	3604.017642	6.503373	-0.030865	3.283528
153.976246	3612.062832	6.508378	-0.030914	3.286996
154.281152	3620.087361	6.513382	-0.030977	3.290454
154.502901	3628.127962	6.518387	-0.031023	3.293912
154.817869	3636.178240	6.523392	-0.031087	3.297374
154.813791	3644.199297	6.528397	-0.031092	3.300807
154.932933	3652.187757	6.533402	-0.031119	3.304228
155.216998	3660.238594	6.538406	-0.031177	3.307678
155.345753	3668.287638	6.543411	-0.031207	3.311118
155.642970	3676.334569	6.548416	-0.031267	3.314560
155.903183	3684.325077	6.553421	-0.031321	3.317972
156.088043	3692.354830	6.558426	-0.031361	3.321395
156.516080	3700.323752	6.563430	-0.031446	3.324798
156.736810	3708.356071	6.568435	-0.031492	3.328216
156.927941	3716.439131	6.573440	-0.031533	3.331651
157.224673	3724.467564	6.578445	-0.031593	3.335064
157.362952	3732.497547	6.583450	-0.031624	3.338467
157.531410	3740.535384	6.588454	-0.031661	3.341872
157.957010	3748.511807	6.593459	-0.031746	3.345256
158.276440	3756.581986	6.598464	-0.031810	3.348673
158.357370	3764.612297	6.603469	-0.031831	3.352061
158.651904	3772.643452	6.608474	-0.031891	3.355453
158.832489	3780.686021	6.613478	-0.031930	3.358843
158.915375	3788.703583	6.618483	-0.031951	3.362215
159.106392	3796.733355	6.623488	-0.031991	3.365593
159.417776	3804.740876	6.628493	-0.032055	3.368962
159.450417	3812.799018	6.633498	-0.032066	3.372339
159.712636	3820.841216	6.638502	-0.032120	3.375714
159.825153	3828.840075	6.643507	-0.032146	3.379062
160.182460	3836.867292	6.648512	-0.032218	3.382428
160.188421	3844.875527	6.653517	-0.032225	3.385770
160.709218	3852.887921	6.658522	-0.032327	3.389128
160.850674	3861.046988	6.663526	-0.032359	3.392531
161.017878	3869.061240	6.668531	-0.032395	3.395871
161.153854	3877.041744	6.673536	-0.032426	3.399192
161.421163	3885.037192	6.678541	-0.032481	3.402521
161.734302	3893.022470	6.683546	-0.032544	3.405844
161.842525	3901.084023	6.688550	-0.032570	3.409189
162.007980	3909.104278	6.693555	-0.032606	3.412514
162.167839	3917.151033	6.698560	-0.032641	3.415848
162.412858	3925.145012	6.703565	-0.032692	3.419159
162.675876	3933.153701	6.708570	-0.032746	3.422474
163.042047	3941.174672	6.713574	-0.032819	3.425794
163.344999	3949.218651	6.718579	-0.032881	3.429118
163.641092	3957.298469	6.723584	-0.032941	3.432453
163.858683	3965.314458	6.728589	-0.032987	3.435756
164.101547	3973.314156	6.733594	-0.033038	3.439050
164.174275	3981.356033	6.738598	-0.033057	3.442352
164.462833	3989.384354	6.743603	-0.033116	3.445653
164.645878	3997.419903	6.748608	-0.033155	3.448950
164.588253	4005.466636	6.753613	-0.033150	3.452241
165.019406	4013.480893	6.758618	-0.033235	3.455531
165.286203	4021.513908	6.763622	-0.033290	3.458821
165.092227	4029.523501	6.768627	-0.033259	3.462082
165.271174	4037.577411	6.773632	-0.033298	3.465371
165.479685	4045.567672	6.778637	-0.033342	3.468631
165.957880	4053.614728	6.783642	-0.033436	3.471921
166.064132	4061.670737	6.788646	-0.033461	3.475199
166.436666	4069.632556	6.793651	-0.033536	3.478444
166.748073	4077.674571	6.798656	-0.033599	3.481716
166.863663	4085.674997	6.803661	-0.033626	3.484962
167.007873	4093.690723	6.808666	-0.033658	3.488213
167.281913	4101.731615	6.813670	-0.033715	3.491474
167.348100	4109.756228	6.818675	-0.033732	3.494720
167.637277	4117.791055	6.823680	-0.033791	3.497973
167.732023	4125.822308	6.828685	-0.033814	3.501216
168.103619	4133.793842	6.833690	-0.033889	3.504440
168.344754	4141.845831	6.838694	-0.033939	3.507690
168.542276	4149.876940	6.843699	-0.033981	3.510927
168.697866	4157.953762	6.848704	-0.034015	3.514178
168.468285	4165.971283	6.853709	-0.033978	3.517390
168.733082	4173.958141	6.858714	-0.034032	3.520602
168.963366	4181.962853	6.863718	-0.034080	3.523818
169.150828	4189.979034	6.868723	-0.034121	3.527033
169.083895	4198.057890	6.873728	-0.034114	3.530263
169.323559	4206.118514	6.878733	-0.034163	3.533492
169.669969	4214.133967	6.883738	-0.034233	3.536704
169.603242	4222.153610	6.888742	-0.034226	3.539901
169.850153	4230.134926	6.893747	-0.034277	3.543090
170.191302	4238.205101	6.898752	-0.034346	3.546314
170.284613	4246.215780	6.903757	-0.034369	3.549504
170.331256	4254.303989	6.908762	-0.034383	3.552721
170.673196	4262.383846	6.913766	-0.034452	3.555940
170.875218	4270.293456	6.918771	-0.034495	3.559084
171.028240	4278.343787	6.923776	-0.034528	3.562280
171.142130	4286.324672	6.928781	-0.034555	3.565445
171.366424	4294.330611	6.933786	-0.034602	3.568620
171.490252	4302.413586	6.938790	-0.034630	3.571819
171.638380	4310.406416	6.943795	-0.034663	3.574981
171.853564	4318.425232	6.948800	-0.034709	3.578152
172.033529	4326.442747	6.953805	-0.034747	3.581318
172.174473	4334.414790	6.958810	-0.034779	3.584463
172.612017	4342.492994	6.963814	-0.034866	3.587655
172.799932	4350.495800	6.968819	-0.034906	3.590808
172.933375	4358.541459	6.973824	-0.034936	3.593973
173.077331	4366.547376	6.978829	-0.034968	3.597120
173.654951	4374.518893	6.983834	-0.035081	3.600263
173.983192	4382.568100	6.988838	-0.035147	3.603426
174.003449	4390.593876	6.993843	-0.035156	3.606569
174.285214	4398.643180	6.998848	-0.035214	3.609726
174.520270	4406.676610	7.003853	-0.035263	3.612872
174.580308	4414.699155	7.008858	-0.035280	3.616007
174.903484	4422.735732	7.013862	-0.035345	3.619151
174.837963	4430.740320	7.018867	-0.035338	3.622270
175.087830	4438.775346	7.023872	-0.035390	3.625406
175.245124	4446.799051	7.028877	-0.035425	3.628533
175.759748	4454.827294	7.033882	-0.035526	3.631668
175.828363	4462.917894	7.038886	-0.035544	3.634813
176.021801	4470.895821	7.043891	-0.035585	3.637915
176.359496	4478.889989	7.048896	-0.035653	3.641024
176.532193	4486.876748	7.053901	-0.035691	3.644123
176.663324	4494.946671	7.058906	-0.035720	3.647251
176.973343	4502.970121	7.063910	-0.035783	3.650363
177.171419	4510.992874	7.068915	-0.035826	3.653468
177.077497	4519.076458	7.073920	-0.035813	3.656587
177.382796	4527.063630	7.078925	-0.035876	3.659677
177.513021	4535.074442	7.083930	-0.035905	3.662768
177.735638	4543.110162	7.088934	-0.035952	3.665869
177.580904	4551.113332	7.093939	-0.035928	3.668945
177.811349	4559.184148	7.098944	-0.035976	3.672054
178.145076	4567.200514	7.103949	-0.036044	3.675142
178.294151	4575.177549	7.108954	-0.036077	3.678208
178.452501	4583.243759	7.113958	-0.036112	3.681306
178.824031	4591.170620	7.118963	-0.036186	3.684353
178.950902	4599.245251	7.123968	-0.036215	3.687448
179.080031	4607.262083	7.128973	-0.036244	3.690518
179.120017	4615.294801	7.133978	-0.036257	3.693589
179.413050	4623.347034	7.138982	-0.036317	3.696672
179.493670	4631.323470	7.143987	-0.036337	3.699718
179.934842	4639.360777	7.148992	-0.036425	3.702793
180.109821	4647.373124	7.153997	-0.036463	3.705850
180.167452	4655.390769	7.159002	-0.036479	3.708903
180.348502	4663.494929	7.164006	-0.036518	3.711990
180.479941	4671.544197	7.169011	-0.036547	3.715052
180.709928	4679.521440	7.174016	-0.036595	3.718087
180.703153	4687.527092	7.179021	-0.036599	3.721124
180.986473	4695.495183	7.184026	-0.036657	3.724151
181.149754	4703.552586	7.189030	-0.036693	3.727207
181.272299	4711.511986	7.194035	-0.036721	3.730222
181.510023	4719.587868	7.199040	-0.036771	3.733282
181.654911	4727.638331	7.204045	-0.036803	3.736327
181.805678	4735.618124	7.209050	-0.036836	3.739343
181.995864	4743.653290	7.214054	-0.036877	3.742379
182.361579	4751.643473	7.219059	-0.036951	3.745399
182.508771	4759.712801	7.224064	-0.036983	3.748441
182.567681	4767.761881	7.229069	-0.037000	3.751471
182.723658	4775.739211	7.234074	-0.037034	3.754475
183.131093	4783.815524	7.239078	-0.037115	3.757518
182.931304	4791.779593	7.244083	-0.037083	3.760503
183.399695	4799.794606	7.249088	-0.037176	3.763520
183.461407	4807.858682	7.254093	-0.037192	3.766544
183.665729	4815.829652	7.259098	-0.037236	3.769534
183.840913	4823.918167	7.264102	-0.037274	3.772564
184.023862	4831.925084	7.269107	-0.037313	3.775562
184.517821	4839.917967	7.274112	-0.037410	3.778559
184.482063	4847.981990	7.279117	-0.037409	3.781568
184.738378	4855.941088	7.284122	-0.037462	3.784543
184.940869	4864.034660	7.289126	-0.037505	3.787563
185.116365	4872.026529	7.294131	-0.037543	3.790543
185.121571	4880.104574	7.299136	-0.037549	3.793549
185.442234	4888.140921	7.304141	-0.037614	3.796544
185.738699	4896.073377	7.309146	-0.037674	3.799498
185.929867	4904.123517	7.314150	-0.037715	3.802490
185.910121	4912.073751	7.319155	-0.037717	3.805438
186.194242	4920.131179	7.324160	-0.037775	3.808431
186.270609	4928.203824	7.329165	-0.037795	3.811422
186.391720	4936.195003	7.334170	-0.037822	3.814382
186.701513	4944.230504	7.339174	-0.037885	3.817359
186.659135	4952.194704	7.344179	-0.037883	3.820301
186.971025	4960.196241	7.349184	-0.037946	3.823262
187.176559	4968.255099	7.354189	-0.037990	3.826239
187.236311	4976.269353	7.359194	-0.038006	3.829194
187.461030	4984.329614	7.364198	-0.038053	3.832167
187.623218	4992.336142	7.369203	-0.038089	3.835117
187.918578	5000.363457	7.374208	-0.038149	3.838076
188.068855	5008.389984	7.379213	-0.038182	3.841028
188.370051	5016.329215	7.384218	-0.038244	3.843949
188.459705	5024.426931	7.389222	-0.038266	3.846922
188.596990	5032.403915	7.394227	-0.038296	3.849849
188.702049	5040.482615	7.399232	-0.038321	3.852811
189.026184	5048.499979	7.404237	-0.038387	3.855752
189.088183	5056.486003	7.409242	-0.038404	3.858674
189.187991	5064.582852	7.414246	-0.038428	3.861635
189.243205	5072.538752	7.419251	-0.038443	3.864542
189.439575	5080.611065	7.424256	-0.038485	3.867492
189.533993	5088.627521	7.429261	-0.038508	3.870417
189.848990	5096.807840	7.434266	-0.038572	3.873404
190.144190	5104.836131	7.439270	-0.038632	3.876332
190.112617	5112.744865	7.444275	-0.038632	3.879209
190.591991	5120.728258	7.449280	-0.038726	3.882120
190.588034	5128.711034	7.454285	-0.038731	3.885020
190.710702	5136.713683	7.459290	-0.038759	3.887927
190.885731	5144.756627	7.464294	-0.038797	3.890848
191.086698	5152.787953	7.469299	-0.038839	3.893763
191.319016	5160.847884	7.474304	-0.038888	3.896686
191.520643	5168.787860	7.479309	-0.038931	3.899563
191.622006	5176.807267	7.484314	-0.038955	3.902465
191.775500	5184.835162	7.489318	-0.038989	3.905369
191.955688	5192.871180	7.494323	-0.039028	3.908274
192.026869	5200.905915	7.499328	-0.039046	3.911174
192.330243	5208.919095	7.504333	-0.039108	3.914069
192.592730	5216.956046	7.509338	-0.039162	3.916969
192.695604	5224.951715	7.514342	-0.039186	3.919850
192.713961	5232.951545	7.519347	-0.039195	3.922728
192.942151	5240.937058	7.524352	-0.039243	3.925603
193.222044	5248.971127	7.529357	-0.039300	3.928494
193.405843	5257.045665	7.534362	-0.039340	3.931395
193.704572	5265.087399	7.539366	-0.039401	3.934285
193.742224	5273.064574	7.544371	-0.039413	3.937145
193.941909	5281.054330	7.549376	-0.039456	3.940010
194.167834	5289.087962	7.554381	-0.039503	3.942889
194.343422	5297.087264	7.559386	-0.039541	3.945753
194.608536	5305.122140	7.564390	-0.039595	3.948629
194.786462	5313.179510	7.569395	-0.039634	3.951509
195.403792	5321.209144	7.574400	-0.039754	3.954385
195.298461	5329.232725	7.579405	-0.039740	3.957244
195.542853	5337.166252	7.584410	-0.039791	3.960075
195.710635	5345.221536	7.589414	-0.039827	3.962946
195.935524	5353.225575	7.594419	-0.039874	3.965798
196.165404	5361.248415	7.599424	-0.039922	3.968654
196.259748	5369.289750	7.604429	-0.039945	3.971513
196.345700	5377.325888	7.609434	-0.039967	3.974367
196.569394	5385.364860	7.614438	-0.040013	3.977223
196.697403	5393.334926	7.619443	-0.040043	3.980050
196.884528	5401.368783	7.624448	-0.040083	3.982900
197.097469	5409.410802	7.629453	-0.040128	3.985750
197.108840	5417.423017	7.634458	-0.040135	3.988584
197.393226	5425.479552	7.639462	-0.040193	3.991437
197.639488	5433.507486	7.644467	-0.040244	3.994277
197.696416	5441.546393	7.649472	-0.040260	3.997115
197.964048	5449.516783	7.654477	-0.040315	3.999931
198.199537	5457.520067	7.659482	-0.040365	4.002756
198.326002	5465.538483	7.664486	-0.040393	4.005582
198.304915	5473.576378	7.669491	-0.040395	4.008411
198.481588	5481.613731	7.674496	-0.040433	4.011241
198.754041	5489.643672	7.679501	-0.040489	4.014068
198.947605	5497.679352	7.684506	-0.040530	4.016893
199.287783	5505.641314	7.689510	-0.040599	4.019693
199.354817	5513.708296	7.694515	-0.040617	4.022523
199.548074	5521.700599	7.699520	-0.040658	4.025327
199.720302	5529.746743	7.704525	-0.040695	4.028148
199.789263	5537.745995	7.709530	-0.040713	4.030949
200.292651	5545.889175	7.714534	-0.040812	4.033805
200.270014	5553.879646	7.719539	-0.040814	4.036597
200.369556	5561.794391	7.724544	-0.040837	4.039363
200.579841	5569.824411	7.729549	-0.040882	4.042168
200.757044	5577.773759	7.734554	-0.040920	4.044944
201.017086	5585.809367	7.739558	-0.040974	4.047748
201.155348	5593.821728	7.744563	-0.041005	4.050541
201.278739	5601.895045	7.749568	-0.041033	4.053352
201.520076	5609.934077	7.754573	-0.041083	4.056152
201.610344	5617.886213	7.759578	-0.041105	4.058917
201.806841	5625.967103	7.764582	-0.041147	4.061726
201.833276	5633.896920	7.769587	-0.041157	4.064479
202.091200	5641.987414	7.774592	-0.041211	4.067289
202.281703	5649.988155	7.779597	-0.041251	4.070065
202.511196	5658.001878	7.784602	-0.041299	4.072844
202.800917	5666.038592	7.789606	-0.041359	4.075629
202.899108	5674.020921	7.794611	-0.041382	4.078392
202.850409	5682.066094	7.799616	-0.041378	4.081172
203.058165	5690.051366	7.804621	-0.041422	4.083933
203.306039	5698.060451	7.809626	-0.041474	4.086701
203.629747	5706.091096	7.814630	-0.041539	4.089475
203.827541	5714.119598	7.819635	-0.041581	4.092246
203.956731	5722.152683	7.824640	-0.041611	4.095015
204.094383	5730.200918	7.829645	-0.041642	4.097787
204.059031	5738.205072	7.834650	-0.041640	4.100540
204.358174	5746.214443	7.839654	-0.041701	4.103297
204.476220	5754.205358	7.844659	-0.041729	4.106044
204.859574	5762.253433	7.849664	-0.041805	4.108812
204.839348	5770.295999	7.854669	-0.041807	4.111571
205.061442	5778.316610	7.859674	-0.041854	4.114323
205.246313	5786.373258	7.864678	-0.041893	4.117086
205.313539	5794.336718	7.869683	-0.041911	4.119814
205.553170	5802.339251	7.874688	-0.041961	4.122555
205.913512	5810.371074	7.879693	-0.042033	4.125305
206.026031	5818.358108	7.884698	-0.042060	4.128036
206.138674	5826.410845	7.889702	-0.042086	4.130787
206.220076	5834.433530	7.894707	-0.042106	4.133526
206.333758	5842.496128	7.899712	-0.042133	4.136276
206.632194	5850.490604	7.904717	-0.042194	4.139004
206.718406	5858.534756	7.909722	-0.042215	4.141745
206.867625	5866.496696	7.914726	-0.042248	4.144456
206.792030	5874.531559	7.919731	-0.042239	4.147188
207.022593	5882.546223	7.924736	-0.042287	4.149915
207.150084	5890.612163	7.929741	-0.042316	4.152656
207.155933	5898.611357	7.934746	-0.042323	4.155371
207.491149	5906.602557	7.939750	-0.042390	4.158086
207.638462	5914.596376	7.944755	-0.042423	4.160797
207.761696	5922.643317	7.949760	-0.042451	4.163525
208.050189	5930.678903	7.954765	-0.042510	4.166248
208.200498	5938.659005	7.959770	-0.042544	4.168950
208.509199	5946.729552	7.964774	-0.042606	4.171682
208.621420	5954.752934	7.969779	-0.042633	4.174394
208.608655	5962.767242	7.974784	-0.042636	4.177100
208.894120	5970.732470	7.979789	-0.042694	4.179791
208.915099	5978.791291	7.984794	-0.042703	4.182508
209.209417	5986.772305	7.989798	-0.042763	4.185201
209.296448	5994.821883	7.994803	-0.042785	4.187913
209.600044	6002.824265	7.999808	-0.042847	4.190609
209.704415	6010.964608	8.004813	-0.042871	4.193348
209.789644	6018.952973	8.009818	-0.042892	4.196034
210.106656	6026.894528	8.014822	-0.042957	4.198705
210.314822	6034.931227	8.019827	-0.043001	4.201405
210.386498	6042.862019	8.024832	-0.043019	4.204066
210.674557	6050.924358	8.029837	-0.043078	4.206772
210.795351	6058.901168	8.034842	-0.043106	4.209446
211.150963	6066.967308	8.039846	-0.043178	4.212150
211.182729	6075.005730	8.044851	-0.043189	4.214840
211.307383	6083.002594	8.049856	-0.043217	4.217515
211.540242	6090.997598	8.054861	-0.043266	4.220189
211.670912	6098.989611	8.059866	-0.043295	4.222859
212.005608	6106.990971	8.064870	-0.043363	4.225533
211.884902	6115.073728	8.069875	-0.043346	4.228228
211.919701	6123.053972	8.074880	-0.043358	4.230888
212.121838	6131.136577	8.079885	-0.043401	4.233582
212.254004	6139.097920	8.084890	-0.043430	4.236234
212.365796	6147.139058	8.089894	-0.043457	4.238910
212.559672	6155.119112	8.094899	-0.043498	4.241565
212.724798	6163.109767	8.099904	-0.043534	4.244221
212.918410	6171.232612	8.104909	-0.043575	4.246920
213.145522	6179.163078	8.109914	-0.043623	4.249554
213.353873	6187.244110	8.114918	-0.043667	4.252236
213.327491	6195.256714	8.119923	-0.043667	4.254891
213.454617	6203.288030	8.124928	-0.043696	4.257552
213.777484	6211.278536	8.129933	-0.043762	4.260200
214.214161	6219.289961	8.134938	-0.043848	4.262854
214.655279	6227.252598	8.139942	-0.043936	4.265490
214.712025	6235.309979	8.144947	-0.043952	4.268153
214.749968	6243.335083	8.149952	-0.043964	4.270803
214.972978	6251.464455	8.154957	-0.044011	4.273487
215.190519	6259.457118	8.159962	-0.044057	4.276124
215.599113	6267.430923	8.164966	-0.044138	4.278756
215.767607	6275.447257	8.169971	-0.044175	4.281397
215.865151	6283.404952	8.174976	-0.044198	4.284017
216.153386	6291.507065	8.179981	-0.044257	4.286685
216.354182	6299.463585	8.184986	-0.044300	4.289302
216.546203	6307.554554	8.189990	-0.044341	4.291961
216.492490	6315.546349	8.194995	-0.044336	4.294585
216.765868	6323.581650	8.200000	-0.044392	4.297224
216.902664	6331.567229	8.205005	-0.044423	4.299843
216.854001	6339.546006	8.210010	-0.044419	4.302458
217.287534	6347.572458	8.215014	-0.044505	4.305090
217.430671	6355.587986	8.220019	-0.044537	4.307714
217.662378	6363.642666	8.225024	-0.044585	4.310351
217.953418	6371.714372	8.230029	-0.044645	4.312992
217.933870	6379.690310	8.235034	-0.044647	4.315597
218.039980	6387.671057	8.240038	-0.044672	4.318204
218.190878	6395.692028	8.245043	-0.044705	4.320822
218.240094	6403.662765	8.250048	-0.044719	4.323422
218.408340	6411.757363	8.255053	-0.044756	4.326061
218.583950	6419.709160	8.260058	-0.044794	4.328653
218.718805	6427.770308	8.265062	-0.044824	4.331278
219.025745	6435.782749	8.270067	-0.044887	4.333886
219.168257	6443.804651	8.275072	-0.044919	4.336495
219.333338	6451.807901	8.280077	-0.044955	4.339097
219.424016	6459.833951	8.285082	-0.044977	4.341704
219.673035	6467.807660	8.290086	-0.045028	4.344293
220.020323	6475.834264	8.295091	-0.045098	4.346899
220.200821	6483.849029	8.300096	-0.045137	4.349498
220.499373	6491.937603	8.305101	-0.045198	4.352120
220.482483	6500.007646	8.310106	-0.045200	4.354733
220.775902	6507.998151	8.315110	-0.045260	4.357320
221.026978	6515.938352	8.320115	-0.045312	4.359889
221.083829	6523.965426	8.325120	-0.045328	4.362483
221.121331	6531.944502	8.330125	-0.045340	4.365061
221.208056	6539.984455	8.335130	-0.045362	4.367656
221.509330	6547.961259	8.340134	-0.045423	4.370231
221.680562	6556.011213	8.345139	-0.045460	4.372827
221.935864	6564.031507	8.350144	-0.045513	4.375413
222.078072	6572.080077	8.355149	-0.045545	4.378006
222.145576	6580.050417	8.360154	-0.045563	4.380571
222.224728	6588.098078	8.365158	-0.045583	4.383160
222.461662	6596.081654	8.370163	-0.045632	4.385727
222.650255	6604.081557	8.375168	-0.045673	4.388298
222.690551	6612.130650	8.380173	-0.045685	4.390883
222.724542	6620.162232	8.385178	-0.045697	4.393460
223.051308	6628.251014	8.390182	-0.045763	4.396056
222.988067	6636.203179	8.395187	-0.045757	4.398604
223.156404	6644.197025	8.400192	-0.045793	4.401165
223.588871	6652.213688	8.405197	-0.045879	4.403733
223.382640	6660.232925	8.410202	-0.045846	4.406298
223.704198	6668.245334	8.415206	-0.045911	4.408861
223.852574	6676.276046	8.420211	-0.045944	4.411428
223.902717	6684.288599	8.425216	-0.045959	4.413987
223.998200	6692.341328	8.430221	-0.045982	4.416558
224.229921	6700.332093	8.435226	-0.046030	4.419108
224.402085	6708.407821	8.440230	-0.046067	4.421683
224.531897	6716.338020	8.445235	-0.046097	4.424211
224.688862	6724.377351	8.450240	-0.046131	4.426771
225.005601	6732.441655	8.455245	-0.046196	4.429339
224.843450	6740.442035	8.460250	-0.046171	4.431883
225.113473	6748.530244	8.465254	-0.046226	4.434455
225.372086	6756.539867	8.470259	-0.046280	4.437001
225.538548	6764.463011	8.475264	-0.046316	4.439517
225.640906	6772.512643	8.480269	-0.046340	4.442072
225.811457	6780.457727	8.485274	-0.046377	4.444592
226.014886	6788.515344	8.490278	-0.046421	4.447147
226.127407	6796.535485	8.495283	-0.046447	4.449688
226.070780	6804.566371	8.500288	-0.046442	4.452230
226.492823	6812.642195	8.505293	-0.046525	4.454787
226.577211	6820.631226	8.510298	-0.046546	4.457314
226.690643	6828.615583	8.515302	-0.046573	4.459838
226.911309	6836.643764	8.520307	-0.046619	4.462374
226.890099	6844.608239	8.525312	-0.046620	4.464888
227.153001	6852.664965	8.530317	-0.046675	4.467431
227.330724	6860.619414	8.535322	-0.046713	4.469940
227.646155	6868.743344	8.540326	-0.046777	4.472501
227.618768	6876.750914	8.545331	-0.046777	4.475023
227.851946	6884.752237	8.550336	-0.046826	4.477543
227.771782	6892.733707	8.555341	-0.046816	4.480054
227.826389	6900.750998	8.560346	-0.046832	4.482575
228.093057	6908.734882	8.565351	-0.046887	4.485084
228.160029	6916.796951	8.570355	-0.046904	4.487617
228.258399	6924.780723	8.575360	-0.046928	4.490123
228.326170	6932.876807	8.580365	-0.046946	4.492663
228.546320	6940.842597	8.585370	-0.046992	4.495161
229.056529	6948.856063	8.590375	-0.047092	4.497674
228.982534	6956.871550	8.595379	-0.047084	4.500184
229.116587	6964.877668	8.600384	-0.047114	4.502690
229.529891	6972.912833	8.605389	-0.047196	4.505205
229.675518	6980.927966	8.610394	-0.047229	4.507711
229.781597	6988.924967	8.615399	-0.047254	4.510211
229.709755	6997.028891	8.620403	-0.047246	4.512741
230.027775	7005.019199	8.625408	-0.047310	4.515236
230.421467	7013.006467	8.630413	-0.047389	4.517729
230.315229	7020.960003	8.635418	-0.047374	4.520208
230.587648	7029.007296	8.640423	-0.047430	4.522716
230.567433	7036.987057	8.645427	-0.047432	4.525202
230.588276	7044.994999	8.650432	-0.047441	4.527694
230.899023	7053.012439	8.655437	-0.047504	4.530189
231.058417	7061.031403	8.660442	-0.047539	4.532682
231.239066	7069.077833	8.665447	-0.047578	4.535183
231.587223	7077.110657	8.670451	-0.047648	4.537679
231.643477	7085.076345	8.675456	-0.047664	4.540151
231.790975	7093.133456	8.680461	-0.047697	4.542651
231.998740	7101.127252	8.685466	-0.047741	4.545130
232.039775	7109.159655	8.690471	-0.047754	4.547619
232.344478	7117.190074	8.695475	-0.047816	4.550107
232.229307	7125.233164	8.700480	-0.047799	4.552596
232.393998	7133.273221	8.705485	-0.047835	4.555084
232.504225	7141.267496	8.710490	-0.047861	4.557556
232.527443	7149.248358	8.715495	-0.047871	4.560022
232.541752	7157.266960	8.720499	-0.047879	4.562499
232.786160	7165.233367	8.725504	-0.047929	4.564958
233.066427	7173.283998	8.730509	-0.047987	4.567443
233.042437	7181.286561	8.735514	-0.047988	4.569910
233.226105	7189.346438	8.740519	-0.048027	4.572394
233.495249	7197.386168	8.745523	-0.048083	4.574871
233.651597	7205.369849	8.750528	-0.048117	4.577329
234.060462	7213.400811	8.755533	-0.048198	4.579800
234.106718	7221.393577	8.760538	-0.048212	4.582258
234.296616	7229.424852	8.765543	-0.048253	4.584727
234.474205	7237.462599	8.770547	-0.048291	4.587196
234.664911	7245.442680	8.775552	-0.048332	4.589646
234.647615	7253.508915	8.780557	-0.048334	4.592121
234.678988	7261.539710	8.785562	-0.048345	4.594584
235.218982	7269.546567	8.790567	-0.048451	4.597039
235.312288	7277.480011	8.795571	-0.048474	4.599469
235.300165	7285.505522	8.800576	-0.048477	4.601927
235.517026	7293.527976	8.805581	-0.048522	4.604382
235.745187	7301.562963	8.810586	-0.048570	4.606839
235.983908	7309.529803	8.815591	-0.048620	4.609275
236.015695	7317.584835	8.820595	-0.048631	4.611736
236.289946	7325.587915	8.825600	-0.048688	4.614180
236.486933	7333.666970	8.830605	-0.048730	4.616646
236.608149	7341.635750	8.835610	-0.048757	4.619076
236.689081	7349.698902	8.840615	-0.048778	4.621535
236.779437	7357.666983	8.845619	-0.048800	4.623963
236.868937	7365.670056	8.850624	-0.048822	4.626400
237.269137	7373.706440	8.855629	-0.048902	4.628846
237.282307	7381.721100	8.860634	-0.048909	4.631284
237.414956	7389.768923	8.865639	-0.048939	4.633731
237.336443	7397.780642	8.870643	-0.048930	4.636166
237.433064	7405.747520	8.875648	-0.048953	4.638586
237.885579	7413.710062	8.880653	-0.049043	4.641003
237.743706	7421.747669	8.885658	-0.049022	4.643442
238.197289	7429.816628	8.890663	-0.049111	4.645889
238.305813	7437.833494	8.895667	-0.049137	4.648319
238.495481	7445.803290	8.900672	-0.049177	4.650733
238.775543	7453.919908	8.905677	-0.049235	4.653190
238.816662	7461.876098	8.910682	-0.049248	4.655598
239.174260	7469.898414	8.915687	-0.049320	4.658024
239.369584	7477.914149	8.920691	-0.049361	4.660447
239.551752	7485.908250	8.925696	-0.049400	4.662862
239.909597	7493.965181	8.930701	-0.049472	4.665295
239.861355	7501.905791	8.935706	-0.049469	4.667692
240.020327	7509.970419	8.940711	-0.049504	4.670124
240.019331	7518.035486	8.945715	-0.049509	4.672556
240.163227	7526.066072	8.950720	-0.049541	4.674976
240.351991	7534.121840	8.955725	-0.049581	4.677402
240.516380	7541.971167	8.960730	-0.049617	4.679765
240.734736	7550.053150	8.965735	-0.049663	4.682196
240.887960	7558.038340	8.970739	-0.049697	4.684597
240.989424	7566.051294	8.975744	-0.049721	4.687006
241.203563	7574.043096	8.980749	-0.049766	4.689406
241.183229	7582.086532	8.985754	-0.049768	4.691821
241.488963	7590.121600	8.990759	-0.049830	4.694232
241.525650	7598.161259	8.995763	-0.049842	4.696644
241.534542	7606.080931	9.000768	-0.049849	4.699018
241.748384	7614.149850	9.005773	-0.049894	4.701435
242.143140	7622.087697	9.010778	-0.049973	4.703812
242.307935	7630.187664	9.015783	-0.050009	4.706236
242.334811	7638.193775	9.020787	-0.050019	4.708631
242.446283	7646.206719	9.025792	-0.050045	4.711027
242.735958	7654.301468	9.030797	-0.050104	4.713445
242.632566	7662.280244	9.035802	-0.050090	4.715829
242.736414	7670.240678	9.040807	-0.050115	4.718206
243.014584	7678.269432	9.045811	-0.050172	4.720601
243.108000	7686.246339	9.050816	-0.050195	4.722980
243.122373	7694.291561	9.055821	-0.050203	4.725378
243.239838	7702.351247	9.060826	-0.050230	4.727779
243.446352	7710.358231	9.065831	-0.050274	4.730163
243.458753	7718.397940	9.070835	-0.050281	4.732556
243.476780	7726.379855	9.075840	-0.050290	4.734931
243.754203	7734.427145	9.080845	-0.050347	4.737323
243.627019	7742.369499	9.085850	-0.050328	4.739684
243.942513	7750.445383	9.090855	-0.050392	4.742082
244.405902	7758.385029	9.095859	-0.050484	4.744438
244.368721	7766.473991	9.100864	-0.050482	4.746838
244.452559	7774.477801	9.105869	-0.050503	4.749212
244.335956	7782.488723	9.110874	-0.050487	4.751587
244.694617	7790.574266	9.115879	-0.050559	4.753982
244.999619	7798.593829	9.120883	-0.050621	4.756356
244.960926	7806.568186	9.125888	-0.050619	4.758716
245.197647	7814.567676	9.130893	-0.050668	4.761082
245.519048	7822.527901	9.135898	-0.050733	4.763435
245.470884	7830.551100	9.140903	-0.050730	4.765806
245.653222	7838.586414	9.145907	-0.050769	4.768179
245.677247	7846.576232	9.150912	-0.050779	4.770538
245.774836	7854.633389	9.155917	-0.050802	4.772916
245.846239	7862.657216	9.160922	-0.050821	4.775282
246.117377	7870.688738	9.165927	-0.050876	4.777649
246.144750	7878.657524	9.170931	-0.050887	4.779997
246.188453	7886.646372	9.175936	-0.050900	4.782350
246.577790	7894.650277	9.180941	-0.050978	4.784704
246.639115	7902.686627	9.185946	-0.050995	4.787069
246.701275	7910.716374	9.190951	-0.051012	4.789430
246.764432	7918.768190	9.195955	-0.051029	4.791796
246.931187	7926.750052	9.200960	-0.051065	4.794141
247.132296	7934.811901	9.205965	-0.051108	4.796507
247.303882	7942.723101	9.210970	-0.051145	4.798828
247.525461	7950.819922	9.215975	-0.051191	4.801203
247.494054	7958.815806	9.220979	-0.051191	4.803547
247.504269	7966.814106	9.225984	-0.051198	4.805891
247.795139	7974.821778	9.230989	-0.051257	4.808235
247.736058	7982.842867	9.235994	-0.051252	4.810584
248.198942	7990.365085	9.240999	-0.051343	4.812783
248.300559	7995.115981	9.246003	-0.051365	4.814173

248.254561	7997.609955	9.251008	-0.051358	4.814902
248.379938	7998.865365	9.256013	-0.051382	4.815269
248.348540	7999.665617	9.261018	-0.051377	4.815503
248.543909	7999.711505	9.266023	-0.051414	4.815515
248.816581	7999.729821	9.271027	-0.051464	4.815519
248.729446	7999.695311	9.276032	-0.051448	4.815510
248.884393	7999.703173	9.281037	-0.051477	4.815511
248.813023	7999.984965	9.286042	-0.051464	4.815594
248.923869	7999.928046	9.291047	-0.051485	4.815577
249.071515	8000.008397	9.296051	-0.051512	4.815600
248.982596	8000.139356	9.301056	-0.051496	4.815638
249.087341	7999.864519	9.306061	-0.051515	4.815557
248.979625	8000.246093	9.311066	-0.051495	4.815670
249.369593	7999.895812	9.316071	-0.051568	4.815565
249.254185	8000.049831	9.321075	-0.051547	4.815611
249.160231	7999.867860	9.326080	-0.051529	4.815558
249.282836	7999.849571	9.331085	-0.051552	4.815552
249.316073	7999.892826	9.336090	-0.051558	4.815565
249.258694	7999.904711	9.341095	-0.051548	4.815568
249.348882	7999.889098	9.346099	-0.051564	4.815563
249.404921	7999.929521	9.351104	-0.051575	4.815575
249.575957	7999.929104	9.356109	-0.051607	4.815574
249.629788	7999.979101	9.361114	-0.051617	4.815588
249.493293	7999.750525	9.366119	-0.051591	4.815522
249.473355	7999.911434	9.371123	-0.051588	4.815569
249.595410	7999.915559	9.376128	-0.051611	4.815570
249.670950	7999.870880	9.381133	-0.051625	4.815557
249.393417	7999.960333	9.386138	-0.051573	4.815584
249.612280	7999.835768	9.391143	-0.051614	4.815547
249.858542	7999.981788	9.396147	-0.051660	4.815588
249.881756	7999.879666	9.401152	-0.051664	4.815558
249.784438	7999.880224	9.406157	-0.051646	4.815559
249.741599	7999.854974	9.411162	-0.051638	4.815552
249.850615	7999.953918	9.416167	-0.051659	4.815580
249.958456	7999.902289	9.421171	-0.051679	4.815564
249.829418	7999.908737	9.426176	-0.051655	4.815567
249.870618	7999.884854	9.431181	-0.051663	4.815560
249.984447	7999.858948	9.436186	-0.051684	4.815552
249.949931	7999.873340	9.441191	-0.051677	4.815556
250.019618	7999.801871	9.446195	-0.051690	4.815535
249.916901	7999.937946	9.451200	-0.051671	4.815575
250.077775	7999.824182	9.456205	-0.051701	4.815541
249.966113	7999.903520	9.461210	-0.051681	4.815565
250.099193	7999.834150	9.466215	-0.051705	4.815544
249.993500	7999.981922	9.471219	-0.051686	4.815587
249.880450	8000.068713	9.476224	-0.051665	4.815613
250.085290	7999.833939	9.481229	-0.051703	4.815544
250.063120	7999.988408	9.486234	-0.051699	4.815589
249.923704	7999.913538	9.491239	-0.051673	4.815568
250.207259	7999.996102	9.496243	-0.051726	4.815591
250.367748	7999.835349	9.501248	-0.051756	4.815543
250.398810	7999.930891	9.506253	-0.051762	4.815571
250.241959	8000.076764	9.511258	-0.051733	4.815614
250.343886	7999.895839	9.516263	-0.051752	4.815561
250.193674	8000.008719	9.521267	-0.051724	4.815594
250.458471	7999.874222	9.526272	-0.051773	4.815554
250.348358	7999.803031	9.531277	-0.051753	4.815533
250.231498	7999.907911	9.536282	-0.051731	4.815565
250.419711	7999.872538	9.541287	-0.051766	4.815553
250.413458	7999.903407	9.546291	-0.051765	4.815562
250.291537	7999.897157	9.551296	-0.051742	4.815561
250.525037	7999.864656	9.556301	-0.051786	4.815551
250.233647	7999.991256	9.561306	-0.051732	4.815589
250.276003	7999.876632	9.566311	-0.051740	4.815555
250.357280	7999.876891	9.571315	-0.051755	4.815555
250.393339	7999.982124	9.576320	-0.051762	4.815586
250.591140	7999.999228	9.581325	-0.051798	4.815590
250.467262	7999.931016	9.586330	-0.051775	4.815570
250.607003	7999.867092	9.591335	-0.051801	4.815551
250.751070	7999.794697	9.596339	-0.051828	4.815529
250.547862	7999.981459	9.601344	-0.051791	4.815585
250.714436	7999.826144	9.606349	-0.051822	4.815538
250.670111	7999.910849	9.611354	-0.051813	4.815563
250.618365	7999.848082	9.616359	-0.051804	4.815545
250.468350	7999.814681	9.621363	-0.051776	4.815536
250.294798	8000.054246	9.626368	-0.051744	4.815607
250.266305	7999.837031	9.631373	-0.051738	4.815544
250.352969	7999.997543	9.636378	-0.051755	4.815590
250.635464	7999.859062	9.641383	-0.051807	4.815548
250.476932	7999.886386	9.646387	-0.051778	4.815557
250.301896	7999.980710	9.651392	-0.051745	4.815586
250.592943	7999.839165	9.656397	-0.051800	4.815543
250.538636	7999.819067	9.661402	-0.051789	4.815537
250.378720	7999.875198	9.666407	-0.051760	4.815554
250.692229	7999.887777	9.671411	-0.051818	4.815557
250.703568	7999.862340	9.676416	-0.051820	4.815549
250.773910	7999.746035	9.681421	-0.051833	4.815515
250.585493	8000.153001	9.686426	-0.051799	4.815635
250.647690	7999.833684	9.691431	-0.051810	4.815541
250.730435	7999.871339	9.696435	-0.051826	4.815552
250.592984	7999.983360	9.701440	-0.051800	4.815585
250.810282	7999.804311	9.706445	-0.051841	4.815532
250.647661	7999.989598	9.711450	-0.051810	4.815587
250.611991	7999.847009	9.716455	-0.051804	4.815545
250.754835	7999.884574	9.721459	-0.051830	4.815555
250.709990	7999.878511	9.726464	-0.051822	4.815554
250.781979	7999.942686	9.731469	-0.051836	4.815572
250.838680	7999.966037	9.736474	-0.051846	4.815579
250.983736	7999.903267	9.741479	-0.051873	4.815560
251.069968	7999.872642	9.746483	-0.051889	4.815550
250.699336	7999.981936	9.751488	-0.051821	4.815584
250.917611	7999.815716	9.756493	-0.051861	4.815534
250.884655	7999.878184	9.761498	-0.051855	4.815553
250.851793	7999.824265	9.766503	-0.051849	4.815537
250.827026	7999.822799	9.771507	-0.051844	4.815537
250.845274	7999.784661	9.776512	-0.051848	4.815526
250.827816	7999.865533	9.781517	-0.051845	4.815549
250.799696	7999.991079	9.786522	-0.051840	4.815586
250.863043	7999.852235	9.791527	-0.051851	4.815545
250.910245	7999.804958	9.796531	-0.051860	4.815531
250.842284	7999.898889	9.801536	-0.051848	4.815559
250.947935	7999.784225	9.806541	-0.051867	4.815525
251.023971	8000.047075	9.811546	-0.051882	4.815601
250.871916	7999.878031	9.816551	-0.051853	4.815553
251.157611	7999.888023	9.821555	-0.051907	4.815554
251.214177	7999.800322	9.826560	-0.051917	4.815528
251.017436	7999.846244	9.831565	-0.051881	4.815543
250.771650	7999.937282	9.836570	-0.051835	4.815571
250.986661	7999.745382	9.841575	-0.051875	4.815513
251.041727	7999.846654	9.846579	-0.051885	4.815543
250.941372	7999.951804	9.851584	-0.051867	4.815574
251.205057	7999.880288	9.856589	-0.051916	4.815552
251.352968	7999.884835	9.861594	-0.051943	4.815552
251.149965	7999.758742	9.866599	-0.051906	4.815517
251.116969	7999.915174	9.871603	-0.051900	4.815562
250.900605	7999.886031	9.876608	-0.051859	4.815555
251.003633	7999.854611	9.881613	-0.051879	4.815545
250.834192	7999.899909	9.886618	-0.051847	4.815559
250.879445	7999.818432	9.891623	-0.051856	4.815535
250.855397	7999.843672	9.896627	-0.051851	4.815543
250.797086	7999.814966	9.901632	-0.051840	4.815535
250.919620	7999.906658	9.906637	-0.051863	4.815561
251.109558	7999.894805	9.911642	-0.051899	4.815557
251.028243	7999.806996	9.916647	-0.051883	4.815531
251.169115	7999.809293	9.921651	-0.051910	4.815531
251.269543	7999.892084	9.926656	-0.051929	4.815555
251.235202	7999.901140	9.931661	-0.051922	4.815558
251.106400	7999.885168	9.936666	-0.051898	4.815554
251.100516	7999.765485	9.941671	-0.051897	4.815519
251.294493	7999.887171	9.946675	-0.051933	4.815553
250.984626	7999.881065	9.951680	-0.051876	4.815553
251.016304	7999.763062	9.956685	-0.051882	4.815518
251.013195	7999.906099	9.961690	-0.051881	4.815560
250.785926	7999.856492	9.966695	-0.051839	4.815547
250.803235	7999.824745	9.971699	-0.051842	4.815537
250.866994	7999.874905	9.976704	-0.051854	4.815552
251.015081	7999.889065	9.981709	-0.051882	4.815555
250.934870	7999.792733	9.986714	-0.051867	4.815528
250.987709	7999.856596	9.991719	-0.051877	4.815546
251.226422	7999.839130	9.996723	-0.051921	4.815540
250.991235	7999.903646	10.001728	-0.051878	4.815560
251.248061	7999.875796	10.006733	-0.051925	4.815550
251.353862	7999.905286	10.011738	-0.051945	4.815558
251.235662	7999.869198	10.016743	-0.051923	4.815548
251.195439	7999.860006	10.021747	-0.051916	4.815546
251.321584	7999.930402	10.026752	-0.051939	4.815566
251.146192	7999.879502	10.031757	-0.051907	4.815552
250.998217	7999.794880	10.036762	-0.051879	4.815528
250.999445	7999.866446	10.041767	-0.051880	4.815549
251.336359	7999.891154	10.046771	-0.051942	4.815554
251.213189	7999.882748	10.051776	-0.051920	4.815552
251.142263	7999.835684	10.056781	-0.051906	4.815539
251.177038	8000.015643	10.061786	-0.051913	4.815592
251.137334	7999.843088	10.066791	-0.051906	4.815541
251.082107	7999.838991	10.071795	-0.051895	4.815540
250.919298	7999.853431	10.076800	-0.051865	4.815545
251.199996	7999.793937	10.081805	-0.051917	4.815527
251.198586	7999.818478	10.086810	-0.051917	4.815534
251.257929	7999.790618	10.091815	-0.051928	4.815525
251.302797	7999.893861	10.096819	-0.051937	4.815555
251.099307	7999.891622	10.101824	-0.051899	4.815556
251.138924	7999.751324	10.106829	-0.051906	4.815514
251.197242	7999.896429	10.111834	-0.051917	4.815557
251.075903	7999.963865	10.116839	-0.051895	4.815577
251.019474	7999.809191	10.121843	-0.051884	4.815532
251.072815	7999.894419	10.126848	-0.051894	4.815557
251.079188	7999.858223	10.131853	-0.051895	4.815546
250.927830	7999.909154	10.136858	-0.051867	4.815562
250.945513	7999.875278	10.141863	-0.051871	4.815552
251.097481	7999.873484	10.146867	-0.051899	4.815550
251.248225	7999.854586	10.151872	-0.051927	4.815544
251.167089	7999.842593	10.156877	-0.051912	4.815541
251.206239	7999.932929	10.161882	-0.051919	4.815567
251.187355	7999.874966	10.166887	-0.051916	4.815550
251.178859	7999.797953	10.171891	-0.051914	4.815528
251.078058	7999.918045	10.176896	-0.051896	4.815563
251.109752	7999.892939	10.181901	-0.051902	4.815556
251.139451	7999.824021	10.186906	-0.051907	4.815536
251.115856	7999.921878	10.191911	-0.051903	4.815564
251.309851	7999.851362	10.196915	-0.051939	4.815543
251.085482	7999.811412	10.201920	-0.051897	4.815532
251.116986	7999.908030	10.206925	-0.051903	4.815560
251.309043	7999.934652	10.211930	-0.051939	4.815567
251.252887	7999.799201	10.216935	-0.051929	4.815528
251.234438	7999.901414	10.221939	-0.051925	4.815558
251.039533	7999.796808	10.226944	-0.051889	4.815528
251.333847	7999.904109	10.231949	-0.051944	4.815558
251.111439	7999.805462	10.236954	-0.051903	4.815530
251.054237	7999.894230	10.241959	-0.051892	4.815557
251.364463	7999.826674	10.246963	-0.051950	4.815535
251.404223	7999.907410	10.251968	-0.051957	4.815559
251.268003	7999.847537	10.256973	-0.051932	4.815542
251.227387	7999.845813	10.261978	-0.051924	4.815542
251.305883	7999.839621	10.266983	-0.051939	4.815539
251.401491	7999.877487	10.271987	-0.051957	4.815550
251.111077	7999.889850	10.276992	-0.051903	4.815555
251.146400	7999.778313	10.281997	-0.051910	4.815522
251.291352	7999.865031	10.287002	-0.051937	4.815547
251.263120	8000.045034	10.292007	-0.051932	4.815600
251.428372	7999.810678	10.297011	-0.051962	4.815530
251.230781	7999.852315	10.302016	-0.051926	4.815543
251.251091	7999.846244	10.307021	-0.051929	4.815542
251.250328	7999.992524	10.312026	-0.051929	4.815584
251.253374	7999.844155	10.317031	-0.051930	4.815541
251.470665	7999.846628	10.322035	-0.051970	4.815541
251.390795	7999.869893	10.327040	-0.051956	4.815548
251.585381	7999.780166	10.332045	-0.051992	4.815521
251.249344	7999.967973	10.337050	-0.051930	4.815577
251.175300	7999.861062	10.342055	-0.051916	4.815546
251.428787	7999.813938	10.347059	-0.051963	4.815531
251.410008	7999.875569	10.352064	-0.051960	4.815549
251.331698	7999.857215	10.357069	-0.051945	4.815544
251.297669	7999.859869	10.362074	-0.051939	4.815545
251.301643	7999.820431	10.367079	-0.051939	4.815534
251.595721	7999.867933	10.372083	-0.051994	4.815546
251.427583	8000.042456	10.377088	-0.051963	4.815598
251.459407	7999.748268	10.382093	-0.051969	4.815512
251.467054	8000.006803	10.387098	-0.051971	4.815587
251.508893	7999.830235	10.392103	-0.051978	4.815536
251.648796	7999.832517	10.397107	-0.052004	4.815536
251.593674	7999.805997	10.402112	-0.051994	4.815528
251.521375	7999.881707	10.407117	-0.051981	4.815551
251.505993	7999.923105	10.412122	-0.051978	4.815563
251.578124	7999.842064	10.417127	-0.051992	4.815539
251.579749	7999.905095	10.422131	-0.051992	4.815557
251.329995	7999.872205	10.427136	-0.051945	4.815549
251.487775	7999.819253	10.432141	-0.051975	4.815532
251.485275	7999.930268	10.437146	-0.051975	4.815565
251.431639	7999.771366	10.442151	-0.051965	4.815519
251.432623	7999.897387	10.447155	-0.051965	4.815556
251.474130	7999.808372	10.452160	-0.051973	4.815529
251.412545	7999.802036	10.457165	-0.051961	4.815528
251.420745	7999.835276	10.462170	-0.051963	4.815537
251.516491	7999.878483	10.467175	-0.051981	4.815550
251.656782	7999.836992	10.472179	-0.052007	4.815537
251.515641	7999.955361	10.477184	-0.051981	4.815572
251.527036	7999.771890	10.482189	-0.051983	4.815518
251.695935	7999.917729	10.487194	-0.052014	4.815560
251.562166	7999.846150	10.492199	-0.051989	4.815540
251.770027	7999.818571	10.497203	-0.052028	4.815531
251.594505	7999.909686	10.502208	-0.051996	4.815558
251.571608	7999.807877	10.507213	-0.051991	4.815529
251.733045	7999.855357	10.512218	-0.052021	4.815542
251.436721	7999.879370	10.517223	-0.051966	4.815550
251.487325	7999.818266	10.522227	-0.051976	4.815532
251.419094	7999.787263	10.527232	-0.051963	4.815523
251.655947	7999.859461	10.532237	-0.052007	4.815543
251.751577	7999.846073	10.537242	-0.052025	4.815539
251.550153	7999.942105	10.542247	-0.051988	4.815568
251.601502	7999.840437	10.547251	-0.051997	4.815538
251.748965	7999.905842	10.552256	-0.052025	4.815557
251.782575	7999.782530	10.557261	-0.052031	4.815520
251.690621	7999.912377	10.562266	-0.052014	4.815559
251.760757	7999.847320	10.567271	-0.052027	4.815539
251.851690	7999.828517	10.572275	-0.052044	4.815533
251.748669	7999.826845	10.577280	-0.052025	4.815533
251.809359	7999.788329	10.582285	-0.052036	4.815522
251.769088	7999.927561	10.587290	-0.052029	4.815563
251.502778	7999.849553	10.592295	-0.051980	4.815541
251.665153	7999.815895	10.597299	-0.052010	4.815531
251.720631	7999.919312	10.602304	-0.052020	4.815561
251.613605	7999.774490	10.607309	-0.052000	4.815519
251.662185	7999.827608	10.612314	-0.052009	4.815534
251.612078	7999.857763	10.617319	-0.052000	4.815543
251.571245	7999.828273	10.622323	-0.051993	4.815535
251.720265	8000.017569	10.627328	-0.052021	4.815589
251.758769	7999.790759	10.632333	-0.052028	4.815523
251.862157	7999.910972	10.637338	-0.052047	4.815557
251.583621	7999.815681	10.642343	-0.051995	4.815531
251.835399	7999.875309	10.647347	-0.052042	4.815547
251.871704	7999.910075	10.652352	-0.052049	4.815557
251.926728	7999.828754	10.657357	-0.052059	4.815533
251.705260	7999.835833	10.662362	-0.052018	4.815536
251.701177	7999.875280	10.667367	-0.052017	4.815548
251.891932	7999.877322	10.672371	-0.052053	4.815547
251.715511	7999.843489	10.677376	-0.052020	4.815538
251.647395	7999.816758	10.682381	-0.052007	4.815531
251.614095	7999.850390	10.687386	-0.052001	4.815541
251.712382	7999.826368	10.692391	-0.052020	4.815533
251.869792	7999.953868	10.697395	-0.052049	4.815570
251.565167	7999.864558	10.702400	-0.051992	4.815545
251.623279	7999.948797	10.707405	-0.052003	4.815570
251.705638	7999.931990	10.712410	-0.052019	4.815564
251.713445	7999.823206	10.717415	-0.052020	4.815532
251.857419	7999.807402	10.722419	-0.052047	4.815527
251.819699	7999.891149	10.727424	-0.052040	4.815552
251.725940	7999.803137	10.732429	-0.052023	4.815527
251.875585	7999.881391	10.737434	-0.052051	4.815549
251.692753	7999.852793	10.742439	-0.052017	4.815541
251.696705	7999.804811	10.747443	-0.052017	4.815527
251.743526	7999.918765	10.752448	-0.052026	4.815560
251.725645	7999.843733	10.757453	-0.052023	4.815538
251.668124	7999.918615	10.762458	-0.052012	4.815561
251.613847	7999.762906	10.767463	-0.052002	4.815515
251.903091	7999.859449	10.772467	-0.052056	4.815542
251.767070	7999.914902	10.777472	-0.052031	4.815559
251.743245	7999.786383	10.782477	-0.052026	4.815522
251.711177	7999.879832	10.787482	-0.052021	4.815549
251.594668	7999.824551	10.792487	-0.051999	4.815533
251.720207	7999.791362	10.797491	-0.052022	4.815523
251.700832	7999.828424	10.802496	-0.052019	4.815534
251.796814	7999.931433	10.807501	-0.052037	4.815564
251.778379	7999.849984	10.812506	-0.052033	4.815540
251.564714	7999.955427	10.817511	-0.051994	4.815572
251.783644	7999.744368	10.822515	-0.052034	4.815509
251.924588	8000.047788	10.827520	-0.052061	4.815597
251.606748	7999.804499	10.832525	-0.052002	4.815528
251.834414	7999.822090	10.837530	-0.052044	4.815532
251.832610	7999.876524	10.842535	-0.052044	4.815547
251.618417	7999.855958	10.847539	-0.052004	4.815542
251.437951	7999.802839	10.852544	-0.051970	4.815528
251.628114	7999.913787	10.857549	-0.052006	4.815559
251.872949	7999.891082	10.862554	-0.052052	4.815552
251.609356	7999.792830	10.867559	-0.052002	4.815524
251.669965	7999.815177	10.872563	-0.052014	4.815530
251.831121	7999.905365	10.877568	-0.052044	4.815556
251.720659	7999.851249	10.882573	-0.052023	4.815541
251.931844	7999.929438	10.887578	-0.052063	4.815562
251.906698	7999.833999	10.892583	-0.052058	4.815535
252.040613	7999.892778	10.897587	-0.052083	4.815551
251.691708	7999.827306	10.902592	-0.052018	4.815534
251.755995	7999.824087	10.907597	-0.052030	4.815532
251.904303	7999.902319	10.912602	-0.052058	4.815555
251.822681	7999.834792	10.917607	-0.052043	4.815535
251.816165	7999.828284	10.922611	-0.052042	4.815533
251.697845	7999.818889	10.927616	-0.052020	4.815531
251.721730	7999.861994	10.932621	-0.052024	4.815544
251.898734	7999.847795	10.937626	-0.052057	4.815539
251.960360	7999.841329	10.942631	-0.052069	4.815537
251.629973	7999.837024	10.947635	-0.052007	4.815537
251.755594	7999.832667	10.952640	-0.052031	4.815535
251.776994	7999.837291	10.957645	-0.052035	4.815536
251.891354	7999.876531	10.962650	-0.052056	4.815547
251.776567	7999.793514	10.967655	-0.052035	4.815523
251.896103	7999.836041	10.972659	-0.052057	4.815535
252.013244	7999.896682	10.977664	-0.052079	4.815552
251.967976	7999.764610	10.982669	-0.052070	4.815514
251.864046	7999.872907	10.987674	-0.052051	4.815546
251.821817	7999.920276	10.992679	-0.052043	4.815560
251.951794	7999.869007	10.997683	-0.052068	4.815545
251.827718	7999.827483	11.002688	-0.052045	4.815533
251.991785	7999.894227	11.007693	-0.052075	4.815552
252.134969	7999.804731	11.012698	-0.052102	4.815525
252.035201	7999.876791	11.017703	-0.052083	4.815547
252.058935	7999.783215	11.022707	-0.052088	4.815519
252.115954	7999.872776	11.027712	-0.052099	4.815545
252.093695	7999.940759	11.032717	-0.052095	4.815565
252.054732	7999.848298	11.037722	-0.052087	4.815538
252.069492	7999.841068	11.042727	-0.052090	4.815536
252.065914	7999.811116	11.047731	-0.052089	4.815527
251.863762	8000.018189	11.052736	-0.052052	4.815589
251.986081	7999.834386	11.057741	-0.052075	4.815534
252.168966	7999.936675	11.062746	-0.052109	4.815563
252.210745	7999.844460	11.067751	-0.052117	4.815536
252.241381	7999.800116	11.072755	-0.052122	4.815523
252.152087	7999.910787	11.077760	-0.052106	4.815556
252.003240	7999.843233	11.082765	-0.052078	4.815537
252.006833	7999.823008	11.087770	-0.052079	4.815531
252.036810	7999.861942	11.092775	-0.052085	4.815542
252.159908	7999.769984	11.097779	-0.052108	4.815515
252.071053	7999.905222	11.102784	-0.052091	4.815555
252.094053	7999.774261	11.107789	-0.052095	4.815516
252.191042	7999.889032	11.112794	-0.052114	4.815549
251.979330	7999.893065	11.117799	-0.052074	4.815552
252.150638	7999.807231	11.122803	-0.052106	4.815526
252.164729	7999.893958	11.127808	-0.052109	4.815551
252.046701	7999.861075	11.132813	-0.052087	4.815542
251.953204	7999.817913	11.137818	-0.052070	4.815530
251.980853	7999.833317	11.142823	-0.052075	4.815534
252.269575	7999.786767	11.147827	-0.052129	4.815519
251.981063	7999.907009	11.152832	-0.052075	4.815556
252.037143	7999.883368	11.157837	-0.052085	4.815548
252.232750	7999.801132	11.162842	-0.052122	4.815523
252.077804	7999.866954	11.167847	-0.052093	4.815543
252.279164	7999.832864	11.172851	-0.052131	4.815532
252.250089	7999.797158	11.177856	-0.052125	4.815522
252.298175	7999.804352	11.182861	-0.052134	4.815524
252.295279	7999.894007	11.187866	-0.052134	4.815550
251.855482	7999.861225	11.192871	-0.052052	4.815543
252.114782	7999.740517	11.197875	-0.052100	4.815506
252.005987	7999.883973	11.202880	-0.052080	4.815549
252.067096	7999.837989	11.207885	-0.052092	4.815535
252.223694	7999.853357	11.212890	-0.052121	4.815539
252.224985	7999.921723	11.217895	-0.052121	4.815559
252.029691	7999.816039	11.222899	-0.052085	4.815529
252.387102	7999.942525	11.227904	-0.052151	4.815564
252.394059	7999.851879	11.232909	-0.052153	4.815537
252.282655	7999.790273	11.237914	-0.052132	4.815520
252.163489	7999.842796	11.242919	-0.052110	4.815536
252.108394	7999.883549	11.247923	-0.052100	4.815548
252.112738	7999.805674	11.252928	-0.052100	4.815525
251.963218	7999.788296	11.257933	-0.052073	4.815521
252.333672	7999.901113	11.262938	-0.052142	4.815552
252.191793	7999.803772	11.267943	-0.052115	4.815524
252.023415	7999.904614	11.272947	-0.052084	4.815555
251.927676	7999.828314	11.277952	-0.052066	4.815533
252.168538	7999.803409	11.282957	-0.052111	4.815524
252.130328	7999.877538	11.287962	-0.052104	4.815546
252.069764	7999.811421	11.292967	-0.052093	4.815527
252.258078	7999.836915	11.297971	-0.052128	4.815534
252.239872	7999.929524	11.302976	-0.052125	4.815561
252.115568	7999.811114	11.307981	-0.052102	4.815527
252.275178	7999.863904	11.312986	-0.052131	4.815542
252.165791	7999.869603	11.317991	-0.052111	4.815544
252.176535	7999.782222	11.322995	-0.052113	4.815518
252.196666	7999.879726	11.328000	-0.052117	4.815547
252.259250	7999.831630	11.333005	-0.052129	4.815532
252.207219	7999.835059	11.338010	-0.052119	4.815533
252.073226	7999.849968	11.343015	-0.052094	4.815538
252.178810	7999.851691	11.348019	-0.052114	4.815538
252.162730	7999.920842	11.353024	-0.052111	4.815559
252.125155	7999.746183	11.358029	-0.052104	4.815508
252.286760	7999.872684	11.363034	-0.052134	4.815544
252.325883	7999.873326	11.368039	-0.052142	4.815544
252.266738	7999.768790	11.373043	-0.052131	4.815514
252.208686	7999.920548	11.378048	-0.052120	4.815558
252.596972	7999.819025	11.383053	-0.052192	4.815527
252.574296	7999.833610	11.388058	-0.052188	4.815531
252.316464	7999.871062	11.393063	-0.052140	4.815543
252.395035	7999.821091	11.398067	-0.052155	4.815528
252.495556	7999.772545	11.403072	-0.052173	4.815514
252.359183	7999.868569	11.408077	-0.052148	4.815542
252.268800	7999.826525	11.413082	-0.052131	4.815531
252.379564	7999.897742	11.418087	-0.052152	4.815551
252.232742	7999.805660	11.423091	-0.052125	4.815525
252.225684	7999.811957	11.428096	-0.052124	4.815527
252.259721	7999.821058	11.433101	-0.052130	4.815529
252.381162	7999.850803	11.438106	-0.052153	4.815537
252.175423	7999.892307	11.443111	-0.052114	4.815550
252.394728	7999.836085	11.448115	-0.052155	4.815533
252.488988	7999.817336	11.453120	-0.052173	4.815527
252.275970	7999.857653	11.458125	-0.052133	4.815540
252.434229	7999.847421	11.463130	-0.052163	4.815536
252.397617	7999.816931	11.468135	-0.052156	4.815527
252.645364	7999.800681	11.473139	-0.052202	4.815521
252.529085	7999.926931	11.478144	-0.052181	4.815559
252.404608	7999.767940	11.483149	-0.052157	4.815513
252.427055	7999.832379	11.488154	-0.052162	4.815532
252.387393	7999.887265	11.493159	-0.052154	4.815548
252.437780	7999.790919	11.498163	-0.052164	4.815519
252.405521	7999.938825	11.503168	-0.052158	4.815563
252.295629	7999.834531	11.508173	-0.052137	4.815533
252.314079	7999.850853	11.513178	-0.052141	4.815537
252.244616	7999.804879	11.518183	-0.052128	4.815524
252.457937	7999.781661	11.523187	-0.052168	4.815517
252.516895	7999.908629	11.528192	-0.052179	4.815553
252.460530	7999.773171	11.533197	-0.052168	4.815514
252.388115	7999.792285	11.538202	-0.052155	4.815520
252.186242	7999.896853	11.543207	-0.052118	4.815552
252.474871	7999.764877	11.548211	-0.052171	4.815512
252.364157	7999.947812	11.553216	-0.052151	4.815566
252.255855	7999.875577	11.558221	-0.052131	4.815545
252.434438	7999.874218	11.563226	-0.052164	4.815544
252.444988	7999.857310	11.568231	-0.052166	4.815539
252.653799	7999.782764	11.573235	-0.052205	4.815516
252.424323	7999.884747	11.578240	-0.052162	4.815547
252.433788	7999.960721	11.583245	-0.052164	4.815569
252.478336	7999.736142	11.588250	-0.052172	4.815503
252.358311	7999.914653	11.593255	-0.052150	4.815556
252.309217	7999.834841	11.598259	-0.052141	4.815533
252.437268	7999.892457	11.603264	-0.052165	4.815549
252.666793	7999.812909	11.608269	-0.052208	4.815525
252.464422	7999.850196	11.613274	-0.052170	4.815537
252.315897	7999.787985	11.618279	-0.052142	4.815519
252.576178	7999.888331	11.623283	-0.052191	4.815547
252.563922	7999.890272	11.628288	-0.052189	4.815548
252.609287	7999.791709	11.633293	-0.052197	4.815519
252.598958	7999.856682	11.638298	-0.052195	4.815538
252.434951	7999.891391	11.643303	-0.052165	4.815549
252.509005	7999.777277	11.648307	-0.052179	4.815515
252.443053	7999.895804	11.653312	-0.052167	4.815550
252.438876	7999.812451	11.658317	-0.052166	4.815526
252.533563	7999.866321	11.663322	-0.052184	4.815541
252.567847	7999.842324	11.668327	-0.052190	4.815534
252.509421	7999.846717	11.673331	-0.052179	4.815535
252.366132	7999.935153	11.678336	-0.052153	4.815562
252.089470	7999.760872	11.683341	-0.052101	4.815512
252.451395	7999.832973	11.688346	-0.052168	4.815532
252.467270	7999.926137	11.693351	-0.052172	4.815559
252.555823	7999.809055	11.698355	-0.052188	4.815524
252.559483	7999.829408	11.703360	-0.052189	4.815530
252.537103	7999.819439	11.708365	-0.052185	4.815527
252.478957	7999.818497	11.713370	-0.052174	4.815527
252.515929	7999.977142	11.718375	-0.052181	4.815573
252.600054	7999.867462	11.723379	-0.052197	4.815541
252.439524	7999.844565	11.728384	-0.052167	4.815535
252.457996	7999.847006	11.733389	-0.052170	4.815536
252.621206	7999.821905	11.738394	-0.052201	4.815528
252.417574	7999.815391	11.743399	-0.052163	4.815527
252.614574	7999.776959	11.748403	-0.052200	4.815514
252.385023	7999.915246	11.753408	-0.052157	4.815556
252.325552	7999.843807	11.758413	-0.052146	4.815535
252.553843	7999.907327	11.763418	-0.052188	4.815553
252.636868	7999.827529	11.768423	-0.052204	4.815529
252.584396	7999.889681	11.773427	-0.052194	4.815547
252.551911	7999.810138	11.778432	-0.052188	4.815524
252.524899	7999.784076	11.783437	-0.052183	4.815517
252.514757	7999.862934	11.788442	-0.052181	4.815540
252.497628	7999.864796	11.793447	-0.052178	4.815541
252.535272	7999.771446	11.798451	-0.052185	4.815513
252.523275	7999.849206	11.803456	-0.052183	4.815536
252.619847	7999.858258	11.808461	-0.052201	4.815538
252.827817	7999.852039	11.813466	-0.052240	4.815535
252.712734	7999.868323	11.818471	-0.052219	4.815541
252.458052	7999.836418	11.823475	-0.052171	4.815532
252.503795	7999.816879	11.828480	-0.052180	4.815527
252.408716	7999.844167	11.833485	-0.052162	4.815535
252.553322	7999.827306	11.838490	-0.052189	4.815529
252.366708	7999.906494	11.843495	-0.052155	4.815553
252.577891	7999.857615	11.848499	-0.052194	4.815538
252.690549	7999.837030	11.853504	-0.052215	4.815532
252.635442	7999.821188	11.858509	-0.052205	4.815527
252.642073	7999.838386	11.863514	-0.052206	4.815532
252.752897	7999.870094	11.868519	-0.052227	4.815541
252.735689	7999.789732	11.873523	-0.052223	4.815518
252.787631	7999.878145	11.878528	-0.052233	4.815543
252.536927	7999.824948	11.883533	-0.052187	4.815529
252.554254	7999.855134	11.888538	-0.052190	4.815537
252.715182	7999.943185	11.893543	-0.052220	4.815562
252.537447	7999.813225	11.898547	-0.052187	4.815525
252.613481	7999.799518	11.903552	-0.052201	4.815521
252.604353	7999.760933	11.908557	-0.052199	4.815510
252.426743	7999.894727	11.913562	-0.052166	4.815550
252.550807	7999.781428	11.918567	-0.052190	4.815516
252.549052	7999.874304	11.923571	-0.052189	4.815543
252.565556	7999.847882	11.928576	-0.052192	4.815535
252.681899	7999.762220	11.933581	-0.052214	4.815510
252.698344	7999.827630	11.938586	-0.052217	4.815529
252.464222	7999.789653	11.943591	-0.052174	4.815519
252.538004	7999.828233	11.948595	-0.052188	4.815530
252.775157	7999.904711	11.953600	-0.052232	4.815551
252.941810	7999.883938	11.958605	-0.052263	4.815544
252.753316	7999.863788	11.963610	-0.052228	4.815539
252.570825	7999.790345	11.968615	-0.052194	4.815518
252.758630	7999.833985	11.973619	-0.052229	4.815530
252.849080	7999.825853	11.978624	-0.052246	4.815528
252.695822	7999.925873	11.983629	-0.052217	4.815557
252.740846	7999.849728	11.988634	-0.052226	4.815535
252.700121	7999.826645	11.993639	-0.052218	4.815528
252.593590	7999.765118	11.998643	-0.052198	4.815511
252.421773	7999.890464	12.003648	-0.052167	4.815548
252.636500	7999.861930	12.008653	-0.052207	4.815539
252.656724	7999.775771	12.013658	-0.052210	4.815514
252.552477	7999.982304	12.018663	-0.052191	4.815575
252.706375	7999.863083	12.023667	-0.052220	4.815539
252.690342	7999.880980	12.028672	-0.052217	4.815544
252.622803	7999.749611	12.033677	-0.052204	4.815506
252.749914	7999.895842	12.038682	-0.052228	4.815548
252.628184	7999.775336	12.043687	-0.052205	4.815514
252.736635	7999.788853	12.048691	-0.052226	4.815517
252.848238	7999.919882	12.053696	-0.052247	4.815555
252.681813	7999.829615	12.058701	-0.052216	4.815529
252.563287	7999.826622	12.063706	-0.052194	4.815529
252.488735	7999.864923	12.068711	-0.052180	4.815541
252.652570	7999.781102	12.073715	-0.052210	4.815515
252.697097	7999.899292	12.078720	-0.052219	4.815550
252.760766	7999.803162	12.083725	-0.052231	4.815521
252.789512	7999.789753	12.088730	-0.052236	4.815517
252.834384	7999.914357	12.093735	-0.052244	4.815553
252.787457	7999.776916	12.098739	-0.052236	4.815513
252.686847	7999.924778	12.103744	-0.052217	4.815557
252.709192	7999.801279	12.108749	-0.052221	4.815521
252.727152	7999.807983	12.113754	-0.052225	4.815523
252.610359	7999.826375	12.118759	-0.052203	4.815529
252.716340	7999.834513	12.123763	-0.052223	4.815531
252.888282	7999.904591	12.128768	-0.052255	4.815550
252.612821	7999.783717	12.133773	-0.052204	4.815516
252.693242	7999.841626	12.138778	-0.052219	4.815533
252.777784	7999.927366	12.143783	-0.052234	4.815557
252.500142	7999.838492	12.148787	-0.052183	4.815533
252.554204	7999.844716	12.153792	-0.052193	4.815534
252.582882	7999.850527	12.158797	-0.052198	4.815536
252.745950	7999.821153	12.163802	-0.052229	4.815527
252.554870	7999.858624	12.168807	-0.052193	4.815538
252.663740	7999.804874	12.173811	-0.052213	4.815522
252.756455	7999.838424	12.178816	-0.052231	4.815532
252.521919	7999.881594	12.183821	-0.052187	4.815545
252.688478	7999.857615	12.188826	-0.052218	4.815537
252.888461	7999.805350	12.193831	-0.052256	4.815521
252.596957	7999.799540	12.198835	-0.052201	4.815521
252.632342	7999.827885	12.203840	-0.052208	4.815529
252.625898	7999.965534	12.208845	-0.052207	4.815569
252.782012	7999.834603	12.213850	-0.052236	4.815530
252.615430	7999.811607	12.218855	-0.052205	4.815524
252.643962	7999.791788	12.223859	-0.052210	4.815518
252.802977	7999.812535	12.228864	-0.052240	4.815524
252.627929	7999.805418	12.233869	-0.052207	4.815523
252.709585	7999.862280	12.238874	-0.052223	4.815539
252.649209	7999.929642	12.243879	-0.052212	4.815559
252.700712	7999.821568	12.248883	-0.052221	4.815527
252.821730	7999.897223	12.253888	-0.052244	4.815548
252.792928	7999.746196	12.258893	-0.052238	4.815504
252.887136	7999.802194	12.263898	-0.052256	4.815520
252.712149	7999.949913	12.268903	-0.052224	4.815564
252.633958	7999.762843	12.273907	-0.052209	4.815510
252.785687	7999.896661	12.278912	-0.052237	4.815548
252.788328	7999.781384	12.283917	-0.052238	4.815515
252.697512	7999.810877	12.288922	-0.052221	4.815524
252.769680	7999.846227	12.293927	-0.052235	4.815534
252.834282	7999.865437	12.298931	-0.052247	4.815539
252.804919	7999.837201	12.303936	-0.052241	4.815531
252.700169	7999.887823	12.308941	-0.052222	4.815546
252.879602	7999.756204	12.313946	-0.052255	4.815507
252.846351	7999.843229	12.318951	-0.052249	4.815532
252.613798	7999.806345	12.323955	-0.052206	4.815523
252.793145	7999.945952	12.328960	-0.052239	4.815563
252.658448	7999.817760	12.333965	-0.052214	4.815526
252.791734	7999.854106	12.338970	-0.052239	4.815536
252.746002	7999.824535	12.343975	-0.052231	4.815528
252.725257	7999.788964	12.348979	-0.052227	4.815517
252.844023	7999.954280	12.353984	-0.052249	4.815565
252.790436	7999.871190	12.358989	-0.052239	4.815541
252.861290	7999.862738	12.363994	-0.052252	4.815538
252.596478	7999.873380	12.368999	-0.052203	4.815542
252.675895	7999.858661	12.374003	-0.052218	4.815538
252.972765	7999.872043	12.379008	-0.052273	4.815540
252.738083	7999.867158	12.384013	-0.052230	4.815540
252.640802	7999.804713	12.389018	-0.052212	4.815522
252.783366	7999.877516	12.394023	-0.052238	4.815543
252.703671	7999.760898	12.399027	-0.052223	4.815509
252.638801	7999.929631	12.404032	-0.052212	4.815559
252.659679	7999.850957	12.409037	-0.052215	4.815536
252.772426	7999.797270	12.414042	-0.052236	4.815519
252.813882	7999.902598	12.419047	-0.052244	4.815550
252.656184	7999.863728	12.424051	-0.052215	4.815539
252.624183	7999.893111	12.429056	-0.052209	4.815548
252.766345	7999.833497	12.434061	-0.052236	4.815530
252.748816	7999.874862	12.439066	-0.052232	4.815542
252.763198	7999.840931	12.444071	-0.052235	4.815532
252.713278	7999.840123	12.449075	-0.052226	4.815532
252.746851	7999.891930	12.454080	-0.052232	4.815547
252.649567	7999.890351	12.459085	-0.052214	4.815547
252.805749	7999.837372	12.464090	-0.052243	4.815531
252.789930	7999.831780	12.469095	-0.052240	4.815529
252.508100	7999.823993	12.474099	-0.052188	4.815528
252.625152	7999.835514	12.479104	-0.052210	4.815531
252.753741	7999.896343	12.484109	-0.052234	4.815548
252.658848	7999.855293	12.489114	-0.052216	4.815537
252.601638	7999.804179	12.494119	-0.052206	4.815522
252.701332	7999.864538	12.499123	-0.052224	4.815539
252.598954	7999.761432	12.504128	-0.052205	4.815510
252.633984	7999.913639	12.509133	-0.052212	4.815554
252.683866	7999.811945	12.514138	-0.052221	4.815524
252.691942	7999.805674	12.519143	-0.052223	4.815522
252.732068	7999.849045	12.524147	-0.052230	4.815535
252.512835	7999.966145	12.529152	-0.052189	4.815570
252.800419	7999.735911	12.534157	-0.052243	4.815501
252.714894	7999.870137	12.539162	-0.052227	4.815541
252.601818	7999.874708	12.544167	-0.052206	4.815543
252.807156	7999.804376	12.549171	-0.052244	4.815521
252.901689	7999.842227	12.554176	-0.052262	4.815532
252.668997	7999.785051	12.559181	-0.052219	4.815516
252.917965	7999.899097	12.564186	-0.052265	4.815548
252.768287	7999.829391	12.569191	-0.052237	4.815529
252.675516	7999.795851	12.574195	-0.052220	4.815519
252.671232	7999.870533	12.579200	-0.052219	4.815541
252.650824	7999.761288	12.584205	-0.052216	4.815509
252.798960	7999.843792	12.589210	-0.052243	4.815533
252.515159	7999.935280	12.594215	-0.052191	4.815561
252.844126	7999.782603	12.599219	-0.052252	4.815515
253.072960	7999.840794	12.604224	-0.052295	4.815531
252.703843	7999.876433	12.609229	-0.052226	4.815543
252.817106	7999.794992	12.614234	-0.052247	4.815518
252.857360	7999.824484	12.619239	-0.052255	4.815527
252.810819	7999.771407	12.624243	-0.052246	4.815512
252.625563	7999.904010	12.629248	-0.052212	4.815551
252.607213	7999.745678	12.634253	-0.052208	4.815505
252.690419	7999.853820	12.639258	-0.052224	4.815536
252.568959	7999.805931	12.644263	-0.052201	4.815523
252.446354	7999.853059	12.649267	-0.052178	4.815537
252.624144	7999.891197	12.654272	-0.052212	4.815547
252.475968	7999.931502	12.659277	-0.052184	4.815560
252.566335	7999.752517	12.664282	-0.052201	4.815507
252.510956	7999.964117	12.669287	-0.052191	4.815569
252.530041	7999.769021	12.674291	-0.052194	4.815512
252.646658	7999.852079	12.679296	-0.052216	4.815536
252.543952	7999.850412	12.684301	-0.052197	4.815536
252.746865	7999.814211	12.689306	-0.052235	4.815524
252.576593	7999.797562	12.694311	-0.052203	4.815520
252.619313	7999.855925	12.699315	-0.052211	4.815537
252.859051	7999.770136	12.704320	-0.052256	4.815511
252.752643	7999.822867	12.709325	-0.052236	4.815527
252.626988	7999.843251	12.714330	-0.052213	4.815533
252.867779	7999.920857	12.719335	-0.052258	4.815555
252.749765	7999.823903	12.724339	-0.052236	4.815527
252.655434	7999.869356	12.729344	-0.052218	4.815541
252.714115	7999.858571	12.734349	-0.052229	4.815537
252.745948	7999.891129	12.739354	-0.052235	4.815547
252.884574	7999.853882	12.744359	-0.052261	4.815535
252.788349	7999.826692	12.749363	-0.052243	4.815528
252.854257	7999.846991	12.754368	-0.052256	4.815533
252.728882	7999.832140	12.759373	-0.052232	4.815530
252.836626	7999.845646	12.764378	-0.052252	4.815533
252.827787	7999.851914	12.769383	-0.052251	4.815535
252.651591	7999.858660	12.774387	-0.052218	4.815538
252.710863	7999.866037	12.779392	-0.052229	4.815540
252.777171	7999.899157	12.784397	-0.052242	4.815549
253.057380	7999.852469	12.789402	-0.052294	4.815534
252.646097	7999.914117	12.794407	-0.052217	4.815554
252.603744	7999.877126	12.799411	-0.052209	4.815543
252.804513	7999.839823	12.804416	-0.052247	4.815532
252.599776	7999.759611	12.809421	-0.052209	4.815509
252.743882	7999.870881	12.814426	-0.052236	4.815541
252.705047	7999.824337	12.819431	-0.052228	4.815528
252.736000	7999.853677	12.824435	-0.052234	4.815536
252.806130	7999.902876	12.829440	-0.052247	4.815550
252.743904	7999.795085	12.834445	-0.052236	4.815519
252.905026	7999.872462	12.839450	-0.052266	4.815541
252.830481	7999.871253	12.844455	-0.052252	4.815541
252.799090	7999.905985	12.849459	-0.052246	4.815551
252.730540	7999.846143	12.854464	-0.052234	4.815534
252.751175	7999.806974	12.859469	-0.052237	4.815522
252.804624	7999.801443	12.864474	-0.052248	4.815520
252.795755	7999.823727	12.869479	-0.052246	4.815527
252.698812	7999.889427	12.874483	-0.052228	4.815547
252.762066	7999.807171	12.879488	-0.052240	4.815522
252.587049	7999.888685	12.884493	-0.052207	4.815547
252.904895	7999.807371	12.889498	-0.052266	4.815522
252.733863	7999.857983	12.894503	-0.052235	4.815537
252.790504	7999.793772	12.899507	-0.052245	4.815518
253.009802	7999.851808	12.904512	-0.052286	4.815534
252.788619	7999.919755	12.909517	-0.052245	4.815555
252.601030	7999.813126	12.914522	-0.052210	4.815525
252.627605	7999.761241	12.919527	-0.052215	4.815509
252.779857	7999.880118	12.924531	-0.052244	4.815543
252.836783	7999.839404	12.929536	-0.052254	4.815531
252.829975	7999.796585	12.934541	-0.052253	4.815519
252.936866	7999.829298	12.939546	-0.052273	4.815528
253.104253	7999.845911	12.944551	-0.052304	4.815532
252.719271	7999.870613	12.949555	-0.052233	4.815541
252.786919	7999.798040	12.954560	-0.052245	4.815519
252.653364	7999.904788	12.959565	-0.052220	4.815551
252.833070	7999.784919	12.964570	-0.052254	4.815515
252.928378	7999.825986	12.969575	-0.052272	4.815527
252.667431	7999.802521	12.974579	-0.052223	4.815521
252.681536	7999.802755	12.979584	-0.052226	4.815521
252.661388	7999.888926	12.984589	-0.052222	4.815547
252.968597	7999.770065	12.989594	-0.052279	4.815510
252.941989	7999.808079	12.994599	-0.052275	4.815522
252.797240	7999.849508	12.999603	-0.052248	4.815534
253.031687	7999.838381	13.004608	-0.052291	4.815530
252.861000	7999.880455	13.009613	-0.052260	4.815543
252.807659	7999.771741	13.014618	-0.052250	4.815512
252.855053	7999.819502	13.019623	-0.052259	4.815525
252.963590	7999.868259	13.024627	-0.052279	4.815539
253.230659	7999.840578	13.029632	-0.052329	4.815530
252.998032	7999.944646	13.034637	-0.052286	4.815561
253.035051	7999.850217	13.039642	-0.052292	4.815533
253.062053	7999.826101	13.044647	-0.052297	4.815526
253.003155	7999.837961	13.049651	-0.052287	4.815530
253.027802	7999.812739	13.054656	-0.052291	4.815523
252.930691	7999.836791	13.059661	-0.052273	4.815530
253.072584	7999.809207	13.064666	-0.052300	4.815521
253.064980	7999.904125	13.069671	-0.052298	4.815549
253.077692	7999.778333	13.074675	-0.052301	4.815512
253.079182	7999.887281	13.079680	-0.052301	4.815544
252.965936	7999.782930	13.084685	-0.052280	4.815514
253.047135	7999.850463	13.089690	-0.052295	4.815533
253.070016	7999.843365	13.094695	-0.052300	4.815531
252.942426	7999.750527	13.099699	-0.052276	4.815505
253.328313	7999.810208	13.104704	-0.052348	4.815520
253.228470	7999.911099	13.109709	-0.052329	4.815550
253.113166	7999.803510	13.114714	-0.052308	4.815519
253.148929	7999.821183	13.119719	-0.052315	4.815524
253.093754	7999.772237	13.124723	-0.052304	4.815510
253.028210	7999.908925	13.129728	-0.052292	4.815551
252.953481	7999.773166	13.134733	-0.052278	4.815511
252.981886	7999.797126	13.139738	-0.052284	4.815518
253.088826	7999.913131	13.144743	-0.052304	4.815552
252.891713	7999.825566	13.149747	-0.052267	4.815527
252.854618	7999.843120	13.154752	-0.052260	4.815532
252.842175	7999.823702	13.159757	-0.052258	4.815527
253.037906	7999.825826	13.164762	-0.052294	4.815526
253.098380	7999.879140	13.169767	-0.052306	4.815542
253.148861	7999.808422	13.174771	-0.052315	4.815521
253.255456	7999.761043	13.179776	-0.052335	4.815506
252.936244	7999.827394	13.184781	-0.052276	4.815527
253.044950	7999.850526	13.189786	-0.052296	4.815533
253.189328	7999.898799	13.194791	-0.052323	4.815547
253.039238	7999.797051	13.199795	-0.052295	4.815518
252.915803	7999.849505	13.204800	-0.052272	4.815534
253.058056	7999.891337	13.209805	-0.052299	4.815545
253.097336	7999.847132	13.214810	-0.052306	4.815532
252.975475	7999.808846	13.219815	-0.052283	4.815522
253.117548	7999.849607	13.224819	-0.052310	4.815533
253.144658	7999.831900	13.229824	-0.052315	4.815528
252.866159	7999.808149	13.234829	-0.052263	4.815522
252.847392	7999.889003	13.239834	-0.052260	4.815546
252.904444	7999.849360	13.244839	-0.052270	4.815534
252.898318	7999.784127	13.249843	-0.052269	4.815515
252.943814	7999.827586	13.254848	-0.052278	4.815527
253.058400	7999.877510	13.259853	-0.052299	4.815541
253.268071	7999.826470	13.264858	-0.052338	4.815525
253.281241	7999.899303	13.269863	-0.052341	4.815547
253.219375	7999.786177	13.274867	-0.052329	4.815514
253.439653	7999.878400	13.279872	-0.052370	4.815540
253.025380	7999.791570	13.284877	-0.052293	4.815516
252.910372	7999.846297	13.289882	-0.052272	4.815533
252.966463	7999.834402	13.294887	-0.052283	4.815529
253.021383	7999.872675	13.299891	-0.052293	4.815540
253.006642	7999.843609	13.304896	-0.052290	4.815532
252.970872	7999.819539	13.309901	-0.052283	4.815525
253.134108	7999.839287	13.314906	-0.052314	4.815530
253.067197	7999.812575	13.319911	-0.052302	4.815522
253.084188	7999.766939	13.324915	-0.052305	4.815509
253.304275	7999.823920	13.329920	-0.052346	4.815524
253.168071	7999.909270	13.334925	-0.052321	4.815550
253.091433	7999.772411	13.339930	-0.052306	4.815510
253.178758	7999.818687	13.344935	-0.052323	4.815523
253.039260	7999.849523	13.349939	-0.052297	4.815533
253.044765	7999.791955	13.354944	-0.052298	4.815516
253.142042	7999.884310	13.359949	-0.052316	4.815543
253.211149	7999.754097	13.364954	-0.052329	4.815504
253.148954	7999.914332	13.369959	-0.052317	4.815552
252.985628	7999.777130	13.374963	-0.052287	4.815512
253.344738	7999.859868	13.379968	-0.052354	4.815535
253.231676	7999.875116	13.384973	-0.052333	4.815540
253.048433	7999.836898	13.389978	-0.052299	4.815529
252.992361	7999.939570	13.394983	-0.052289	4.815560
252.933878	7999.795533	13.399987	-0.052278	4.815518
252.891592	7999.843969	13.404992	-0.052270	4.815532
253.040229	7999.835717	13.409997	-0.052298	4.815529
253.176423	7999.827261	13.415002	-0.052323	4.815526
253.225905	7999.839818	13.420007	-0.052332	4.815529
253.076452	7999.915341	13.425011	-0.052305	4.815552
253.197171	7999.792375	13.430016	-0.052327	4.815516
253.131562	7999.782769	13.435021	-0.052315	4.815513
253.145769	7999.888721	13.440026	-0.052318	4.815544
253.283819	7999.851465	13.445031	-0.052343	4.815532
253.155428	7999.845107	13.450035	-0.052319	4.815531
253.026891	7999.865443	13.455040	-0.052296	4.815538
252.976766	7999.848614	13.460045	-0.052286	4.815533
253.078574	7999.799021	13.465050	-0.052305	4.815518
252.958248	7999.846187	13.470055	-0.052283	4.815532
252.782475	7999.889246	13.475059	-0.052250	4.815546
253.011424	7999.832113	13.480064	-0.052293	4.815528
253.254347	7999.809378	13.485069	-0.052338	4.815520
253.234198	7999.835751	13.490074	-0.052335	4.815528
253.314862	7999.846680	13.495079	-0.052350	4.815531
253.172014	7999.831545	13.500083	-0.052323	4.815527
253.233674	7999.875267	13.505088	-0.052335	4.815540
253.144818	7999.846061	13.510093	-0.052318	4.815532
253.340516	7999.865271	13.515098	-0.052355	4.815536
253.302299	7999.904164	13.520103	-0.052348	4.815548
253.000148	7999.819160	13.525107	-0.052291	4.815524
253.128273	7999.967546	13.530112	-0.052315	4.815567
252.938918	7999.841665	13.535117	-0.052280	4.815531
252.909855	7999.855078	13.540122	-0.052275	4.815535
253.049825	7999.868041	13.545127	-0.052301	4.815538
253.211545	7999.782049	13.550131	-0.052331	4.815513
252.951961	7999.855779	13.555136	-0.052283	4.815535
252.986424	7999.832853	13.560141	-0.052289	4.815528
253.181018	7999.860587	13.565146	-0.052326	4.815536
253.228368	7999.951062	13.570151	-0.052334	4.815562
253.045865	7999.850921	13.575155	-0.052300	4.815533
253.259437	7999.853336	13.580160	-0.052340	4.815533
253.392344	7999.848031	13.585165	-0.052365	4.815531
253.281124	7999.861174	13.590170	-0.052344	4.815535
253.317339	7999.876719	13.595175	-0.052351	4.815540
253.238565	7999.811371	13.600179	-0.052337	4.815521
253.116361	7999.856370	13.605184	-0.052314	4.815535
253.067458	7999.826747	13.610189	-0.052305	4.815526
253.257737	7999.807426	13.615194	-0.052340	4.815520
253.393950	7999.875856	13.620199	-0.052366	4.815539
253.242899	7999.854179	13.625203	-0.052338	4.815533
253.334670	7999.857815	13.630208	-0.052355	4.815534
253.220384	7999.848483	13.635213	-0.052334	4.815532
253.093367	7999.861369	13.640218	-0.052310	4.815536
253.124178	7999.871487	13.645223	-0.052316	4.815539
253.041164	7999.812476	13.650227	-0.052300	4.815522
253.178739	7999.888403	13.655232	-0.052326	4.815544
253.219954	7999.875197	13.660237	-0.052334	4.815540
253.203678	7999.857851	13.665242	-0.052331	4.815535
253.008261	7999.892048	13.670247	-0.052295	4.815546
253.033492	7999.887125	13.675251	-0.052299	4.815544
253.209561	7999.908151	13.680256	-0.052332	4.815549
253.223685	7999.880622	13.685261	-0.052335	4.815541
253.140877	7999.822682	13.690266	-0.052319	4.815525
253.177624	7999.888424	13.695271	-0.052326	4.815544
253.258793	7999.927126	13.700275	-0.052342	4.815555
253.211862	7999.828125	13.705280	-0.052333	4.815526
253.024570	7999.853911	13.710285	-0.052298	4.815534
253.216698	7999.830349	13.715290	-0.052334	4.815527
253.257890	7999.875874	13.720295	-0.052342	4.815540
253.220668	7999.810135	13.725299	-0.052335	4.815521
253.377696	7999.874632	13.730304	-0.052364	4.815539
253.304577	7999.847818	13.735309	-0.052350	4.815531
253.399043	7999.860040	13.740314	-0.052368	4.815534
253.304416	7999.885200	13.745319	-0.052351	4.815542
253.213509	7999.865570	13.750323	-0.052334	4.815537
253.273717	7999.867624	13.755328	-0.052345	4.815537
253.191062	7999.878029	13.760333	-0.052330	4.815541
253.406011	7999.906095	13.765338	-0.052370	4.815548
253.225246	7999.923445	13.770343	-0.052336	4.815554
252.916807	7999.860763	13.775347	-0.052279	4.815537
253.162403	7999.882921	13.780352	-0.052325	4.815542
253.213146	7999.864531	13.785357	-0.052334	4.815537
253.115645	7999.902458	13.790362	-0.052316	4.815548
253.045464	7999.874624	13.795367	-0.052303	4.815540
253.028469	7999.785722	13.800371	-0.052300	4.815514
253.073546	7999.806750	13.805376	-0.052308	4.815520
253.141284	7999.813197	13.810381	-0.052321	4.815522
253.168622	7999.864904	13.815386	-0.052326	4.815537
253.215238	7999.873143	13.820391	-0.052335	4.815539
253.082704	7999.815461	13.825395	-0.052310	4.815523
253.271067	7999.849501	13.830400	-0.052345	4.815532
253.105283	7999.935437	13.835405	-0.052315	4.815558
253.442372	7999.880066	13.840410	-0.052377	4.815540
253.322065	7999.884518	13.845415	-0.052355	4.815542
252.978411	7999.838348	13.850419	-0.052291	4.815530
253.225889	7999.898979	13.855424	-0.052337	4.815547
253.008391	7999.886899	13.860429	-0.052297	4.815544
253.059146	7999.835406	13.865434	-0.052306	4.815529
253.155213	7999.854061	13.870439	-0.052324	4.815534
253.178393	7999.828815	13.875443	-0.052329	4.815526
253.264428	7999.951956	13.880448	-0.052345	4.815562
253.230783	7999.837153	13.885453	-0.052338	4.815528
253.255364	7999.868526	13.890458	-0.052343	4.815537
253.288873	7999.878687	13.895463	-0.052349	4.815540
253.261007	7999.849407	13.900467	-0.052344	4.815532
253.360140	7999.883062	13.905472	-0.052363	4.815541
253.206286	7999.868814	13.910477	-0.052334	4.815538
253.252591	7999.890930	13.915482	-0.052343	4.815544
253.402691	7999.861345	13.920487	-0.052371	4.815535
253.219414	7999.802837	13.925491	-0.052337	4.815518
253.030872	7999.856366	13.930496	-0.052302	4.815535
253.120132	7999.933642	13.935501	-0.052318	4.815557
253.232605	7999.771031	13.940506	-0.052339	4.815509
253.264297	7999.859115	13.945511	-0.052345	4.815535
253.061720	7999.887856	13.950515	-0.052308	4.815544
253.154805	7999.808221	13.955520	-0.052325	4.815520
253.224605	7999.943911	13.960525	-0.052338	4.815560
253.264640	7999.803613	13.965530	-0.052346	4.815518
253.204736	7999.841084	13.970535	-0.052335	4.815530
253.195305	7999.829190	13.975539	-0.052333	4.815526
253.465245	7999.842134	13.980544	-0.052383	4.815529
253.366677	7999.825584	13.985549	-0.052365	4.815524
253.394083	7999.783321	13.990554	-0.052370	4.815512
253.490540	7999.960024	13.995559	-0.052388	4.815563
253.291855	7999.812633	14.000563	-0.052351	4.815521
253.246677	7999.886652	14.005568	-0.052343	4.815543
253.203202	7999.893423	14.010573	-0.052335	4.815545
253.206304	7999.871054	14.015578	-0.052335	4.815538
253.338392	7999.897771	14.020583	-0.052360	4.815546
253.284400	7999.825351	14.025587	-0.052350	4.815525
253.220547	7999.838198	14.030592	-0.052338	4.815529
253.215986	7999.872299	14.035597	-0.052337	4.815539
253.202430	7999.773842	14.040602	-0.052335	4.815510
253.065702	7999.829284	14.045607	-0.052309	4.815527
252.836251	7999.916318	14.050611	-0.052267	4.815553
253.073991	7999.877481	14.055616	-0.052311	4.815541
253.092666	7999.829737	14.060621	-0.052315	4.815527
253.069208	7999.843242	14.065626	-0.052310	4.815531
253.195021	7999.918977	14.070631	-0.052334	4.815552
253.421642	7999.875689	14.075635	-0.052376	4.815539
253.244944	7999.920868	14.080640	-0.052343	4.815553
253.232478	7999.877956	14.085645	-0.052341	4.815540
253.160653	7999.788161	14.090650	-0.052328	4.815514
253.433883	7999.879111	14.095655	-0.052379	4.815540
253.225536	7999.887469	14.100659	-0.052340	4.815543
253.262825	7999.850707	14.105664	-0.052347	4.815532
253.206843	7999.882903	14.110669	-0.052337	4.815542
252.929938	7999.815396	14.115674	-0.052285	4.815523
253.213452	7999.849917	14.120679	-0.052338	4.815532
253.417109	7999.825475	14.125683	-0.052376	4.815524
253.394681	7999.881711	14.130688	-0.052372	4.815541
253.241901	7999.867481	14.135693	-0.052343	4.815537
253.254064	7999.808953	14.140698	-0.052346	4.815520
253.439003	7999.945451	14.145703	-0.052380	4.815559
253.270284	7999.859415	14.150707	-0.052349	4.815535
253.492317	7999.884394	14.155712	-0.052390	4.815541
253.329649	7999.865731	14.160717	-0.052360	4.815536
253.218152	7999.823342	14.165722	-0.052339	4.815524
253.317464	7999.873018	14.170727	-0.052358	4.815538
253.366815	7999.773449	14.175731	-0.052367	4.815509
253.203703	7999.911753	14.180736	-0.052337	4.815550
253.197445	7999.853992	14.185741	-0.052336	4.815533
253.244678	7999.820595	14.190746	-0.052344	4.815523
253.335948	7999.900040	14.195751	-0.052362	4.815546
253.271511	7999.810364	14.200755	-0.052350	4.815520
253.300634	7999.823657	14.205760	-0.052355	4.815524
253.275070	7999.832856	14.210765	-0.052350	4.815527
253.323713	7999.793076	14.215770	-0.052359	4.815515
253.298655	7999.859947	14.220775	-0.052355	4.815535
253.243529	7999.841968	14.225779	-0.052345	4.815530
253.532862	7999.860568	14.230784	-0.052399	4.815534
253.460544	7999.964044	14.235789	-0.052385	4.815564
253.406383	7999.820075	14.240794	-0.052375	4.815523
253.595933	7999.896849	14.245799	-0.052410	4.815544
253.117880	7999.589006	14.250803	-0.052321	4.815456

253.226789	7996.342782	14.255808	-0.052340	4.814507
253.203327	7990.706376	14.260813	-0.052332	4.812858
253.313134	7983.910107	14.265818	-0.052348	4.810869
253.194730	7976.671561	14.270823	-0.052321	4.808751
253.108783	7969.044524	14.275827	-0.052300	4.806518
253.132335	7961.225667	14.280832	-0.052299	4.804227
253.088997	7953.401006	14.285837	-0.052286	4.801933
252.986445	7945.361040	14.290842	-0.052262	4.799576
253.007460	7937.481144	14.295847	-0.052261	4.797264
252.879610	7929.371088	14.300851	-0.052232	4.794884
252.829740	7921.413957	14.305856	-0.052217	4.792547
252.690794	7913.412732	14.310861	-0.052186	4.790196
252.673979	7905.405528	14.315866	-0.052178	4.787842
252.883149	7897.428743	14.320871	-0.052212	4.785495
252.754681	7889.427869	14.325875	-0.052183	4.783141
252.793177	7881.388708	14.330880	-0.052185	4.780774
252.594905	7873.443634	14.335885	-0.052143	4.778434
252.410408	7865.365038	14.340890	-0.052103	4.776054
252.588138	7857.433865	14.345895	-0.052131	4.773715
252.426695	7849.332951	14.350899	-0.052096	4.771326
252.385381	7841.408971	14.355904	-0.052083	4.768987
252.486558	7833.373328	14.360909	-0.052097	4.766614
252.349849	7825.376818	14.365914	-0.052066	4.764251
252.204677	7817.454979	14.370919	-0.052034	4.761910
252.141267	7809.332258	14.375923	-0.052017	4.759508
252.117197	7801.444075	14.380928	-0.052007	4.757174
252.180374	7793.337252	14.385933	-0.052014	4.754774
252.054122	7785.309331	14.390938	-0.051985	4.752397
252.100642	7777.343189	14.395943	-0.051989	4.750036
252.003670	7769.333143	14.400947	-0.051965	4.747661
252.134490	7761.353744	14.405952	-0.051985	4.745294
251.926344	7753.332722	14.410957	-0.051941	4.742914
251.834919	7745.302280	14.415962	-0.051919	4.740529
251.823982	7737.359718	14.420967	-0.051911	4.738170
251.882891	7729.289497	14.425971	-0.051917	4.735771
251.888444	7721.343538	14.430976	-0.051913	4.733408
251.521349	7713.263796	14.435981	-0.051840	4.731005
251.303863	7705.269363	14.440986	-0.051794	4.728626
251.529314	7697.296637	14.445991	-0.051831	4.726250
251.410424	7689.291305	14.450995	-0.051803	4.723865
251.299290	7681.315262	14.456000	-0.051778	4.721487
251.322087	7673.293139	14.461005	-0.051777	4.719094
251.227351	7665.377659	14.466010	-0.051754	4.716732
251.451234	7657.358980	14.471015	-0.051790	4.714337
251.157328	7649.274440	14.476019	-0.051731	4.711923
251.273759	7641.289177	14.481024	-0.051747	4.709536
251.210687	7633.324339	14.486029	-0.051730	4.707154
251.010309	7625.224878	14.491034	-0.051688	4.704731
251.151338	7617.330170	14.496039	-0.051709	4.702367
251.122584	7609.305880	14.501043	-0.051698	4.699964
251.132850	7601.368256	14.506048	-0.051695	4.697585
251.122601	7593.326257	14.511053	-0.051688	4.695174
251.010395	7585.289846	14.516058	-0.051662	4.692764
250.936135	7577.250566	14.521063	-0.051643	4.690351
250.781583	7569.261762	14.526067	-0.051609	4.687952
251.010597	7561.311495	14.531072	-0.051646	4.685564
250.705481	7553.368508	14.536077	-0.051585	4.683176
250.414689	7545.269949	14.541082	-0.051525	4.680741
250.650949	7537.315326	14.546087	-0.051564	4.678347
250.575707	7529.271935	14.551091	-0.051545	4.675926
250.625512	7521.198105	14.556096	-0.051549	4.673494
250.545324	7513.138238	14.561101	-0.051529	4.671065
250.442861	7505.184983	14.566106	-0.051505	4.668667
250.484687	7497.249906	14.571111	-0.051507	4.666273
250.382063	7489.200444	14.576115	-0.051483	4.663843
250.276742	7481.255466	14.581120	-0.051458	4.661444
250.197649	7473.249642	14.586125	-0.051438	4.659025
250.158921	7465.260539	14.591130	-0.051426	4.656610
250.287886	7457.272004	14.596135	-0.051445	4.654194
250.261048	7449.194295	14.601139	-0.051435	4.651749
250.232112	7441.214648	14.606144	-0.051424	4.649333
250.099405	7433.212116	14.611149	-0.051394	4.646909
249.973720	7425.187062	14.616154	-0.051366	4.644476
250.059071	7417.271708	14.621159	-0.051376	4.642076
249.977096	7409.198591	14.626163	-0.051356	4.639626
249.895514	7401.267546	14.631168	-0.051336	4.637219
249.707479	7393.219236	14.636173	-0.051295	4.634774
249.646902	7385.170297	14.641178	-0.051279	4.632328
249.741397	7377.164835	14.646183	-0.051291	4.629894
249.669280	7369.186983	14.651187	-0.051273	4.627467
249.596958	7361.177463	14.656192	-0.051254	4.625029
249.509072	7353.221386	14.661197	-0.051233	4.622606
249.511223	7345.184544	14.666202	-0.051228	4.620157
249.452211	7337.234881	14.671207	-0.051212	4.617733
249.255062	7329.193232	14.676211	-0.051170	4.615280
249.278216	7321.188637	14.681216	-0.051169	4.612837
249.377091	7313.137150	14.686221	-0.051182	4.610379
249.216804	7305.185074	14.691226	-0.051147	4.607949
249.192554	7297.146290	14.696231	-0.051138	4.605492
249.043750	7289.177240	14.701235	-0.051105	4.603055
248.970007	7281.191995	14.706240	-0.051086	4.600611
248.955162	7273.205855	14.711245	-0.051078	4.598166
248.984552	7265.163798	14.716250	-0.051078	4.595702
249.044898	7257.132107	14.721255	-0.051084	4.593241
249.034241	7249.079397	14.726259	-0.051077	4.590771
249.091932	7241.132612	14.731264	-0.051083	4.588333
249.013817	7233.124263	14.736269	-0.051063	4.585874
248.670981	7225.126997	14.741274	-0.050994	4.583418
248.846291	7217.161216	14.746279	-0.051022	4.580970
248.852776	7209.136169	14.751283	-0.051018	4.578502
248.650247	7201.127251	14.756288	-0.050975	4.576038
248.709034	7193.121886	14.761293	-0.050981	4.573574
248.715730	7185.118974	14.766298	-0.050977	4.571109
248.644278	7177.137885	14.771303	-0.050958	4.568649
248.519310	7169.140077	14.776307	-0.050930	4.566183
248.502714	7161.107765	14.781312	-0.050922	4.563705
248.464291	7153.143628	14.786317	-0.050909	4.561247
248.303468	7145.142910	14.791322	-0.050874	4.558776
248.218749	7137.172513	14.796327	-0.050853	4.556313
248.130792	7129.116633	14.801331	-0.050832	4.553822
248.283906	7121.070055	14.806336	-0.050855	4.551333
248.261898	7113.072097	14.811341	-0.050846	4.548858
248.308002	7105.097293	14.816346	-0.050849	4.546388
248.330555	7097.114856	14.821351	-0.050848	4.543915
248.153405	7089.137914	14.826355	-0.050810	4.541442
248.009260	7081.140043	14.831360	-0.050778	4.538961
247.986367	7073.170001	14.836365	-0.050769	4.536487
247.847818	7065.137712	14.841370	-0.050738	4.533993
248.049069	7057.080562	14.846375	-0.050770	4.531490
247.762015	7049.074252	14.851379	-0.050711	4.529000
247.806446	7041.091242	14.856384	-0.050715	4.526517
247.604144	7033.144447	14.861389	-0.050672	4.524044
247.524260	7025.125010	14.866394	-0.050652	4.521547
247.819927	7017.136278	14.871399	-0.050702	4.519058
247.506960	7009.160528	14.876403	-0.050638	4.516571
247.540802	7001.126524	14.881408	-0.050639	4.514066
247.535840	6993.041282	14.886413	-0.050633	4.511542
247.471700	6985.052024	14.891418	-0.050616	4.509048
247.505176	6977.062398	14.896423	-0.050617	4.506552
247.346067	6969.050906	14.901427	-0.050582	4.504047
247.209552	6961.043741	14.906432	-0.050552	4.501542
247.108304	6953.087650	14.911437	-0.050528	4.499052
247.065150	6945.090619	14.916442	-0.050515	4.496548
247.029941	6937.084046	14.921447	-0.050503	4.494039
247.080332	6929.007461	14.926451	-0.050507	4.491508
246.932404	6921.034888	14.931456	-0.050474	4.489007
246.786528	6913.074760	14.936461	-0.050442	4.486508
246.793365	6905.039046	14.941466	-0.050438	4.483985
246.766749	6897.092650	14.946471	-0.050428	4.481488
246.804929	6889.061648	14.951475	-0.050430	4.478964
246.897829	6881.085184	14.956480	-0.050442	4.476455
246.726865	6873.062509	14.961485	-0.050405	4.473930
246.602087	6865.010223	14.966490	-0.050377	4.471394
246.547115	6857.029129	14.971495	-0.050361	4.468879
246.414364	6849.031677	14.976499	-0.050331	4.466357
246.414168	6840.991725	14.981504	-0.050326	4.463821
246.521860	6833.070765	14.986509	-0.050341	4.461322
246.333175	6824.983858	14.991514	-0.050301	4.458767
246.272210	6817.053201	14.996519	-0.050284	4.456261
246.359559	6809.008680	15.001523	-0.050295	4.453719
246.316158	6800.999994	15.006528	-0.050282	4.451185
246.173589	6792.993231	15.011533	-0.050251	4.448650
245.909429	6784.972981	15.016538	-0.050196	4.446109
246.217796	6777.030571	15.021543	-0.050248	4.443594
246.137758	6769.047587	15.026547	-0.050228	4.441063
245.905879	6761.063404	15.031552	-0.050180	4.438529
246.052523	6753.054037	15.036557	-0.050202	4.435987
245.933784	6744.960573	15.041562	-0.050175	4.433416
245.873531	6736.976115	15.046567	-0.050159	4.430879
245.944319	6728.955102	15.051571	-0.050167	4.428329
245.871416	6720.954531	15.056576	-0.050148	4.425783
245.668476	6712.973280	15.061581	-0.050105	4.423241
245.481271	6705.002348	15.066586	-0.050065	4.420702
245.761552	6696.978021	15.071591	-0.050112	4.418146
245.791160	6688.970916	15.076595	-0.050112	4.415592
245.610521	6680.980531	15.081600	-0.050073	4.413042
245.596284	6672.977545	15.086605	-0.050066	4.410487
245.562906	6664.979518	15.091610	-0.050054	4.407932
245.477399	6656.994806	15.096615	-0.050033	4.405379
245.300126	6648.978211	15.101619	-0.049995	4.402815
245.142036	6640.997257	15.106624	-0.049960	4.400260
245.072834	6633.032186	15.111629	-0.049942	4.397709
244.907303	6624.991577	15.116634	-0.049906	4.395132
245.103242	6617.000171	15.121639	-0.049938	4.392572
245.126699	6608.946294	15.126643	-0.049937	4.389989
244.991745	6600.957318	15.131648	-0.049907	4.387424
245.049838	6592.992969	15.136653	-0.049912	4.384867
244.971904	6585.007526	15.141658	-0.049893	4.382300
245.031189	6577.009747	15.146663	-0.049899	4.379729
244.896089	6569.017304	15.151667	-0.049868	4.377157
244.921838	6560.989792	15.156672	-0.049868	4.374574
244.913737	6553.000602	15.161677	-0.049861	4.372000
244.697349	6544.954214	15.166682	-0.049816	4.369406
244.736906	6537.046214	15.171687	-0.049818	4.366856
244.613155	6528.999912	15.176691	-0.049790	4.364259
244.183737	6521.016627	15.181696	-0.049705	4.361679
244.388260	6512.975509	15.186701	-0.049738	4.359083
244.488357	6504.978844	15.191706	-0.049751	4.356499
244.524609	6496.944749	15.196711	-0.049753	4.353901
244.114494	6488.865670	15.201715	-0.049671	4.351284
244.123599	6480.900627	15.206720	-0.049668	4.348705
244.230059	6472.949859	15.211725	-0.049682	4.346129
244.238740	6464.971152	15.216730	-0.049679	4.343543
244.270541	6456.973624	15.221735	-0.049680	4.340949
244.221775	6448.963353	15.226739	-0.049665	4.338348
244.070458	6440.978370	15.231744	-0.049632	4.335754
244.159622	6432.976703	15.236749	-0.049643	4.333154
243.903532	6424.903846	15.241754	-0.049591	4.330527
243.850989	6416.999380	15.246759	-0.049576	4.327955
243.763090	6408.934578	15.251763	-0.049554	4.325329
243.769557	6400.959787	15.256768	-0.049550	4.322731
243.827718	6392.968519	15.261773	-0.049556	4.320127
243.447204	6384.957610	15.266778	-0.049480	4.317511
243.712581	6376.962680	15.271783	-0.049524	4.314904
243.639737	6368.922983	15.276787	-0.049505	4.312278
243.489874	6360.896709	15.281792	-0.049472	4.309654
243.428920	6352.963026	15.286797	-0.049456	4.307060
243.257525	6344.906081	15.291802	-0.049419	4.304423
243.325606	6336.939938	15.296807	-0.049426	4.301816
243.280053	6328.909888	15.301811	-0.049413	4.299185
243.404206	6320.986346	15.306816	-0.049431	4.296589
243.444211	6312.943043	15.311821	-0.049433	4.293952
243.062697	6304.896082	15.316826	-0.049357	4.291308
243.145253	6296.903500	15.321831	-0.049367	4.288684
243.162190	6288.916483	15.326835	-0.049365	4.286060
243.045922	6280.910201	15.331840	-0.049338	4.283427
242.866954	6272.951293	15.336845	-0.049300	4.280807
242.735898	6264.956281	15.341850	-0.049270	4.278175
242.721758	6256.955642	15.346855	-0.049262	4.275539
242.760579	6248.876179	15.351859	-0.049264	4.272877
242.794029	6240.841633	15.356864	-0.049265	4.270228
242.853231	6232.897455	15.361869	-0.049271	4.267607
242.644877	6224.846181	15.366874	-0.049227	4.264946
242.551230	6216.949027	15.371879	-0.049205	4.262336
242.521786	6208.874702	15.376883	-0.049194	4.259667
242.629756	6200.889453	15.381888	-0.049209	4.257026
242.569940	6192.922217	15.386893	-0.049193	4.254388
242.583707	6184.890074	15.391898	-0.049190	4.251728
242.471911	6176.901299	15.396903	-0.049164	4.249079
242.204265	6168.888989	15.401907	-0.049109	4.246420
242.169713	6160.911915	15.406912	-0.049098	4.243772
242.242626	6152.942425	15.411917	-0.049106	4.241127
242.100134	6144.928629	15.416922	-0.049074	4.238463
242.208685	6136.934295	15.421927	-0.049089	4.235806
242.078391	6128.938735	15.426931	-0.049060	4.233145
242.001503	6120.901700	15.431936	-0.049040	4.230469
242.097074	6112.918128	15.436941	-0.049053	4.227810
242.110544	6104.903584	15.441946	-0.049050	4.225139
242.025342	6096.943838	15.446951	-0.049029	4.222483
241.757806	6088.930079	15.451955	-0.048974	4.219806
241.870374	6080.948373	15.456960	-0.048990	4.217142
241.982223	6072.939939	15.461965	-0.049006	4.214467
241.919224	6064.916692	15.466970	-0.048989	4.211784
241.777427	6056.936461	15.471975	-0.048957	4.209112
241.689190	6048.953179	15.476979	-0.048936	4.206438
241.640308	6040.916031	15.481984	-0.048922	4.203745
241.610697	6032.979351	15.486989	-0.048911	4.201085
241.297776	6024.960817	15.491994	-0.048848	4.198392
241.414524	6016.959970	15.496999	-0.048864	4.195707
241.334073	6008.855272	15.502003	-0.048844	4.192984
241.158234	6000.825804	15.507008	-0.048806	4.190284
241.324550	5992.861996	15.512013	-0.048832	4.187607
240.992010	5984.857291	15.517018	-0.048765	4.184910
241.195737	5976.938606	15.522023	-0.048798	4.182245
241.150163	5968.899710	15.527027	-0.048784	4.179536
240.949811	5960.942445	15.532032	-0.048741	4.176851
240.996596	5952.937764	15.537037	-0.048745	4.174151
240.897376	5944.851619	15.542042	-0.048721	4.171420
240.964944	5936.897311	15.547047	-0.048729	4.168733
240.956684	5928.900822	15.552051	-0.048722	4.166030
240.975655	5920.886465	15.557056	-0.048720	4.163319
240.896361	5912.930480	15.562061	-0.048701	4.160625
240.843074	5904.939172	15.567066	-0.048686	4.157918
240.514226	5896.935013	15.572071	-0.048619	4.155201
240.457611	5888.891787	15.577075	-0.048603	4.152472
240.551979	5880.832959	15.582080	-0.048616	4.149738
240.380714	5872.903636	15.587085	-0.048579	4.147043
240.178482	5864.862168	15.592090	-0.048536	4.144308
240.253280	5856.952989	15.597095	-0.048545	4.141619
240.254416	5848.899307	15.602099	-0.048540	4.138879
240.254546	5840.863834	15.607104	-0.048535	4.136143
240.357890	5832.897734	15.612109	-0.048549	4.133430
240.092518	5824.864193	15.617114	-0.048494	4.130687
240.247008	5816.918633	15.622119	-0.048518	4.127978
240.084728	5808.884746	15.627123	-0.048482	4.125234
240.165225	5800.889335	15.632128	-0.048492	4.122503
240.032505	5792.928111	15.637133	-0.048462	4.119780
240.008814	5784.961756	15.642138	-0.048453	4.117054
239.859145	5776.895104	15.647143	-0.048420	4.114291
239.845417	5768.844301	15.652147	-0.048412	4.111533
239.696869	5760.854102	15.657152	-0.048379	4.108792
239.853373	5752.879515	15.662157	-0.048403	4.106059
239.862614	5744.853082	15.667162	-0.048400	4.103304
239.764515	5736.880699	15.672167	-0.048376	4.100564
239.735041	5728.927381	15.677171	-0.048366	4.097831
239.481603	5720.927300	15.682176	-0.048313	4.095076
239.437651	5712.926342	15.687181	-0.048300	4.092321
239.303857	5704.882671	15.692186	-0.048270	4.089549
239.349085	5696.948839	15.697191	-0.048273	4.086816
239.436995	5688.923588	15.702195	-0.048284	4.084049
239.321417	5680.929942	15.707200	-0.048258	4.081289
239.249790	5672.984282	15.712205	-0.048239	4.078544
239.370587	5664.934212	15.717210	-0.048257	4.075764
239.244120	5656.900490	15.722215	-0.048228	4.072984
239.217998	5648.902509	15.727219	-0.048218	4.070216
239.227603	5640.929257	15.732224	-0.048215	4.067456
239.225707	5632.918662	15.737229	-0.048209	4.064680
238.978302	5624.954264	15.742234	-0.048158	4.061915
239.107124	5616.939351	15.747239	-0.048177	4.059136
239.086057	5608.956787	15.752243	-0.048168	4.056363
238.930298	5600.938616	15.757248	-0.048133	4.053575
238.909046	5592.904232	15.762253	-0.048124	4.050781
238.771206	5584.938626	15.767258	-0.048093	4.048008
238.591388	5576.922956	15.772263	-0.048055	4.045214
238.694105	5568.978810	15.777267	-0.048069	4.042448
238.644842	5560.915877	15.782272	-0.048054	4.039636
238.723815	5552.989042	15.787277	-0.048064	4.036871
238.479504	5544.896525	15.792282	-0.048013	4.034042
238.613619	5536.813941	15.797287	-0.048033	4.031220
238.491363	5528.857025	15.802291	-0.048005	4.028436
238.218638	5520.881027	15.807296	-0.047949	4.025641
238.291203	5512.943660	15.812301	-0.047958	4.022863
238.274282	5504.891884	15.817306	-0.047949	4.020042
238.138219	5496.927604	15.822311	-0.047919	4.017248
238.238881	5488.919258	15.827315	-0.047932	4.014439
238.166393	5480.860220	15.832320	-0.047914	4.011609
238.123357	5472.881976	15.837325	-0.047901	4.008805
237.917888	5464.866953	15.842330	-0.047857	4.005983
237.900490	5456.928985	15.847335	-0.047849	4.003190
237.904140	5448.913182	15.852339	-0.047844	4.000368
237.826144	5440.945742	15.857344	-0.047825	3.997559
237.732797	5432.955436	15.862349	-0.047802	3.994740
237.868153	5424.900141	15.867354	-0.047822	3.991900
237.634681	5416.884375	15.872359	-0.047773	3.989066
237.620824	5408.885412	15.877363	-0.047766	3.986240
237.642953	5400.881631	15.882368	-0.047765	3.983410
237.687437	5392.928352	15.887373	-0.047768	3.980596
237.444263	5384.937800	15.892378	-0.047717	3.977763
237.437329	5376.936616	15.897383	-0.047711	3.974927
237.453083	5368.950637	15.902387	-0.047709	3.972096
237.289582	5360.883902	15.907392	-0.047673	3.969230
237.462472	5352.973092	15.912397	-0.047700	3.966424
237.271429	5344.938615	15.917402	-0.047659	3.963565
237.107759	5337.002602	15.922407	-0.047624	3.960740
237.123796	5329.003128	15.927411	-0.047622	3.957894
237.078321	5320.972963	15.932416	-0.047608	3.955033
237.315623	5312.945357	15.937421	-0.047647	3.952176
237.105643	5304.909478	15.942426	-0.047603	3.949306
236.983722	5296.976637	15.947431	-0.047575	3.946473
236.978058	5288.987022	15.952435	-0.047569	3.943619
236.718259	5280.963399	15.957440	-0.047515	3.940746
236.767593	5273.008897	15.962445	-0.047519	3.937902
236.702897	5264.954223	15.967450	-0.047502	3.935017
236.844907	5256.943920	15.972455	-0.047523	3.932151
236.567140	5248.978802	15.977459	-0.047466	3.929290
236.513828	5240.987397	15.982464	-0.047451	3.926422
236.762420	5233.004813	15.987469	-0.047493	3.923561
236.419708	5224.994626	15.992474	-0.047424	3.920677
236.306726	5217.037778	15.997479	-0.047397	3.917814
236.423918	5209.007345	16.002483	-0.047414	3.914927
236.416958	5200.961446	16.007488	-0.047408	3.912030
236.327797	5193.002846	16.012493	-0.047386	3.909160
236.265809	5184.952660	16.017498	-0.047369	3.906256
236.283618	5177.008118	16.022503	-0.047367	3.903389
236.429756	5168.993575	16.027507	-0.047389	3.900498
236.122286	5161.026834	16.032512	-0.047327	3.897613
236.316307	5152.984517	16.037517	-0.047358	3.894708
235.923196	5144.957577	16.042522	-0.047280	3.891795
235.935700	5136.986832	16.047527	-0.047277	3.888908
236.154900	5128.966242	16.052531	-0.047312	3.886005
235.999706	5120.988756	16.057536	-0.047278	3.883108
235.844365	5113.000969	16.062541	-0.047244	3.880205
235.948437	5105.013872	16.067546	-0.047258	3.877305
235.765913	5096.985521	16.072551	-0.047219	3.874383
235.570243	5088.790768	16.077555	-0.047178	3.871397
235.610992	5080.849259	16.082560	-0.047180	3.868506
235.780737	5072.893792	16.087565	-0.047207	3.865611
235.472999	5064.943834	16.092570	-0.047144	3.862705
235.577360	5056.949134	16.097575	-0.047158	3.859790
235.481167	5048.986021	16.102579	-0.047135	3.856879
235.277178	5040.967479	16.107584	-0.047092	3.853944
235.430186	5032.973710	16.112589	-0.047116	3.851023
235.115982	5024.992370	16.117594	-0.047052	3.848095
235.290742	5016.981390	16.122599	-0.047079	3.845164
235.200368	5009.069638	16.127603	-0.047057	3.842262
235.112538	5001.022571	16.132608	-0.047036	3.839307
235.024340	4993.095651	16.137613	-0.047014	3.836395
234.934036	4985.044129	16.142618	-0.046992	3.833434
234.819562	4977.004489	16.147623	-0.046966	3.830475
234.896817	4969.029708	16.152627	-0.046975	3.827542
234.813952	4961.015955	16.157632	-0.046954	3.824588
234.772823	4953.106787	16.162637	-0.046942	3.821672
234.668170	4945.082982	16.167642	-0.046917	3.818710
234.645387	4937.089460	16.172647	-0.046908	3.815758
234.483255	4929.080663	16.177651	-0.046872	3.812796
234.342222	4921.054151	16.182656	-0.046841	3.809825
234.363028	4913.084389	16.187661	-0.046840	3.806876
234.363347	4905.054584	16.192666	-0.046834	3.803902
234.428673	4897.112288	16.197671	-0.046841	3.800960
234.410237	4889.118799	16.202675	-0.046833	3.797995
234.386515	4881.094048	16.207680	-0.046823	3.795016
234.490209	4873.042847	16.212685	-0.046837	3.792027
234.191358	4865.053837	16.217690	-0.046777	3.789050
234.270698	4857.059537	16.222695	-0.046786	3.786077
234.220883	4849.101861	16.227699	-0.046772	3.783113
233.971761	4841.088750	16.232704	-0.046720	3.780121
233.917908	4833.132230	16.237709	-0.046705	3.777152
233.867676	4825.114053	16.242714	-0.046691	3.774158
233.769981	4817.078417	16.247719	-0.046667	3.771154
233.871969	4809.095496	16.252723	-0.046681	3.768172
233.560385	4801.076579	16.257728	-0.046618	3.765165
233.718915	4793.137057	16.262733	-0.046642	3.762196
233.583801	4785.103554	16.267738	-0.046612	3.759182
233.667949	4777.120441	16.272743	-0.046622	3.756190
233.744015	4769.103420	16.277747	-0.046631	3.753182
233.580533	4761.046197	16.282752	-0.046596	3.750152
233.500469	4753.115712	16.287757	-0.046576	3.747168
233.546036	4745.092496	16.292762	-0.046579	3.744151
233.213668	4737.150807	16.297767	-0.046512	3.741152
233.325838	4729.147938	16.302771	-0.046528	3.738139
233.249514	4721.107104	16.307776	-0.046508	3.735104
233.388982	4713.134426	16.312781	-0.046529	3.732098
233.036213	4705.130788	16.317786	-0.046458	3.729066
232.979560	4697.135607	16.322791	-0.046443	3.726042
232.918577	4689.187637	16.327795	-0.046426	3.723033
232.834483	4681.173440	16.332800	-0.046405	3.719996
233.130895	4673.218789	16.337805	-0.046455	3.716988
232.801582	4665.160209	16.342810	-0.046389	3.713923
232.746380	4657.080034	16.347815	-0.046373	3.710854
232.759096	4649.123730	16.352819	-0.046371	3.707832
232.765115	4641.104593	16.357824	-0.046367	3.704782
232.762739	4633.178708	16.362829	-0.046361	3.701766
232.630189	4625.168665	16.367834	-0.046331	3.698712
232.585086	4617.204593	16.372839	-0.046318	3.695674
232.497296	4609.191008	16.377843	-0.046296	3.692615
232.230923	4601.204063	16.382848	-0.046241	3.689558
232.478636	4593.225777	16.387853	-0.046282	3.686516
232.470213	4585.223647	16.392858	-0.046276	3.683455
232.508328	4577.211222	16.397863	-0.046278	3.680389
232.273230	4569.270942	16.402867	-0.046229	3.677341
232.120763	4561.217881	16.407872	-0.046195	3.674249
232.257512	4553.228698	16.412877	-0.046216	3.671187
232.066137	4545.236528	16.417882	-0.046175	3.668112
232.159408	4537.206764	16.422887	-0.046187	3.665028
232.141163	4529.256167	16.427891	-0.046178	3.661969
232.019670	4521.230898	16.432896	-0.046151	3.658875
231.819752	4513.276929	16.437901	-0.046108	3.655805
231.884522	4505.238844	16.442906	-0.046115	3.652706
231.861023	4497.217643	16.447911	-0.046106	3.649609
231.952166	4489.256780	16.452915	-0.046117	3.646536
231.659162	4481.258839	16.457920	-0.046058	3.643436
231.746083	4473.291596	16.462925	-0.046069	3.640354
231.696789	4465.305050	16.467930	-0.046054	3.637260
231.593922	4457.279946	16.472935	-0.046030	3.634146
231.746036	4449.249645	16.477939	-0.046053	3.631034
231.515697	4441.229570	16.482944	-0.046005	3.627913
231.345770	4433.277310	16.487949	-0.045968	3.624818
231.568076	4425.282719	16.492954	-0.046005	3.621714
231.220965	4417.316551	16.497959	-0.045935	3.618603
231.101128	4409.357363	16.502963	-0.045907	3.615498
231.074191	4401.292876	16.507968	-0.045897	3.612352
231.212805	4393.294828	16.512973	-0.045918	3.609234
231.060393	4385.330744	16.517978	-0.045884	3.606118
230.906947	4377.355335	16.522983	-0.045851	3.602995
230.936920	4369.371395	16.527987	-0.045851	3.599871
230.914576	4361.386979	16.532992	-0.045842	3.596743
230.817991	4353.393377	16.537997	-0.045819	3.593606
230.802827	4345.363550	16.543002	-0.045811	3.590455
230.904264	4337.343474	16.548007	-0.045824	3.587308
230.852485	4329.378028	16.553011	-0.045810	3.584175
230.611750	4321.386521	16.558016	-0.045760	3.581024
230.655925	4313.424178	16.563021	-0.045763	3.577890
230.440916	4305.403029	16.568026	-0.045718	3.574722
230.591074	4297.385261	16.573031	-0.045740	3.571564
230.519745	4289.406612	16.578035	-0.045722	3.568412
230.348415	4281.391094	16.583040	-0.045685	3.565239
230.445444	4273.440280	16.588045	-0.045698	3.562097
230.702338	4265.413655	16.593050	-0.045740	3.558927
230.465322	4257.444936	16.598055	-0.045691	3.555763
230.225263	4249.372705	16.603059	-0.045641	3.552554
229.940317	4241.325384	16.608064	-0.045583	3.549351
230.309138	4233.356686	16.613069	-0.045647	3.546196
230.144299	4225.387891	16.618074	-0.045611	3.543022
229.926555	4217.414617	16.623079	-0.045565	3.539842
229.923506	4209.463747	16.628083	-0.045559	3.536675
229.848383	4201.431546	16.633088	-0.045540	3.533470
229.722579	4193.425371	16.638093	-0.045512	3.530270
229.715930	4185.440111	16.643098	-0.045505	3.527080
229.826277	4177.449265	16.648103	-0.045521	3.523889
229.719475	4169.493122	16.653107	-0.045496	3.520701
229.492093	4161.481802	16.658112	-0.045448	3.517485
229.692413	4153.480874	16.663117	-0.045480	3.514284
229.464242	4145.470374	16.668122	-0.045433	3.511062
229.387010	4137.464231	16.673127	-0.045413	3.507844
229.633744	4129.451274	16.678131	-0.045454	3.504630
229.492444	4121.515986	16.683136	-0.045422	3.501433
229.409704	4113.564092	16.688141	-0.045402	3.498227
229.279334	4105.545063	16.693146	-0.045372	3.494991
229.270599	4097.557275	16.698151	-0.045366	3.491767
229.441326	4089.553541	16.703155	-0.045392	3.488540
229.183877	4081.546769	16.708160	-0.045339	3.485295
229.192664	4073.605278	16.713165	-0.045336	3.482082
229.187189	4065.599049	16.718170	-0.045329	3.478839
228.975066	4057.606635	16.723175	-0.045285	3.475592
228.953965	4049.588954	16.728179	-0.045276	3.472338
228.952316	4041.574953	16.733184	-0.045270	3.469083
228.767770	4033.585359	16.738189	-0.045231	3.465829
228.702453	4025.603035	16.743194	-0.045213	3.462579
228.727860	4017.598758	16.748199	-0.045213	3.459319
228.652000	4009.664491	16.753203	-0.045194	3.456082
228.541337	4001.636501	16.758208	-0.045168	3.452802
228.604669	3993.589936	16.763213	-0.045175	3.449518
228.631582	3985.641728	16.768218	-0.045174	3.446269
228.554447	3977.645389	16.773223	-0.045155	3.442994
228.523340	3969.672004	16.778227	-0.045144	3.439727
228.404600	3961.683668	16.783232	-0.045117	3.436447
228.297852	3953.674668	16.788237	-0.045092	3.433157
228.186175	3945.659371	16.793242	-0.045066	3.429860
228.194785	3937.678397	16.798247	-0.045062	3.426579
228.211433	3929.699102	16.803251	-0.045060	3.423295
227.919362	3921.711241	16.808256	-0.045001	3.419994
227.947694	3913.739577	16.813261	-0.045001	3.416708
228.196376	3905.701391	16.818266	-0.045042	3.413398
227.857099	3897.720436	16.823271	-0.044974	3.410089
227.750447	3889.743887	16.828275	-0.044949	3.406786
227.833099	3881.731456	16.833280	-0.044959	3.403472
227.787762	3873.774389	16.838285	-0.044945	3.400172
227.952602	3865.775871	16.843290	-0.044971	3.396860
227.625001	3857.774566	16.848295	-0.044905	3.393527
227.775830	3849.699733	16.853299	-0.044928	3.390176
227.527536	3841.727230	16.858304	-0.044876	3.386850
227.638440	3833.757044	16.863309	-0.044892	3.383535
227.594673	3825.785268	16.868314	-0.044878	3.380210
227.383889	3817.822082	16.873319	-0.044834	3.376880
227.243715	3809.842168	16.878323	-0.044803	3.373542
227.282983	3801.784759	16.883328	-0.044805	3.370175
227.199977	3793.841280	16.888333	-0.044784	3.366847
227.026280	3785.858349	16.893338	-0.044747	3.363497
227.094173	3777.848572	16.898343	-0.044754	3.360140
227.084391	3769.890625	16.903347	-0.044747	3.356799
227.020608	3761.851697	16.908352	-0.044730	3.353419
226.938782	3753.863272	16.913357	-0.044710	3.350056
226.957889	3745.862308	16.918362	-0.044708	3.346688
226.722305	3737.881147	16.923367	-0.044659	3.343316
226.729132	3729.930693	16.928371	-0.044655	3.339962
226.621715	3721.940560	16.933376	-0.044630	3.336584
227.055623	3713.901652	16.938381	-0.044706	3.333201
226.866879	3705.898712	16.943386	-0.044666	3.329808
226.510681	3697.954089	16.948391	-0.044594	3.326429
226.431822	3689.971226	16.953395	-0.044574	3.323041
226.304259	3681.973643	16.958400	-0.044545	3.319641
226.377532	3674.013564	16.963405	-0.044554	3.316262
226.301182	3665.987523	16.968410	-0.044535	3.312845
226.120934	3657.959973	16.973415	-0.044496	3.309420
226.138103	3650.003788	16.978419	-0.044494	3.306030
226.078968	3642.006982	16.983424	-0.044478	3.302616
226.004335	3634.043973	16.988429	-0.044459	3.299212
225.887377	3626.063088	16.993434	-0.044432	3.295795
225.806402	3618.055961	16.998439	-0.044411	3.292365
226.045010	3610.029206	17.003443	-0.044451	3.288935
225.930405	3602.064376	17.008448	-0.044424	3.285514
226.041480	3594.097690	17.013453	-0.044440	3.282098
225.940861	3586.103958	17.018458	-0.044416	3.278659
226.056509	3578.088171	17.023463	-0.044432	3.275215
225.867186	3570.108486	17.028467	-0.044392	3.271770
225.701836	3562.083731	17.033472	-0.044356	3.268304
225.859275	3554.103894	17.038477	-0.044380	3.264866
225.514408	3546.170399	17.043482	-0.044311	3.261425
225.416040	3538.155035	17.048487	-0.044287	3.257954
225.495862	3530.157838	17.053491	-0.044297	3.254495
225.160252	3522.146884	17.058496	-0.044229	3.251009
225.122935	3514.173979	17.063501	-0.044217	3.247548
225.310719	3506.184474	17.068506	-0.044247	3.244085
225.094923	3498.223580	17.073511	-0.044202	3.240614
225.129490	3490.251663	17.078515	-0.044203	3.237146
225.141153	3482.199473	17.083520	-0.044200	3.233637
225.200800	3474.157984	17.088525	-0.044206	3.230131
224.993382	3466.190873	17.093530	-0.044162	3.226643
225.283435	3458.181630	17.098535	-0.044211	3.223154
225.266545	3450.233243	17.103539	-0.044203	3.219674
225.052271	3442.279253	17.108544	-0.044158	3.216180
224.964956	3434.294313	17.113549	-0.044136	3.212674
224.724530	3426.297056	17.118554	-0.044086	3.209153
224.596599	3418.292381	17.123559	-0.044057	3.205629
224.534183	3410.371905	17.128563	-0.044041	3.202140
224.265786	3402.371998	17.133568	-0.043986	3.198605
224.451234	3394.369015	17.138573	-0.044015	3.195083
224.425551	3386.350378	17.143578	-0.044005	3.191541
224.161771	3378.356347	17.148583	-0.043951	3.187996
224.165637	3370.376037	17.153587	-0.043946	3.184465
223.986305	3362.408771	17.158592	-0.043908	3.180928
224.128423	3354.390013	17.163597	-0.043929	3.177378
224.147594	3346.408155	17.168602	-0.043927	3.173834
224.037965	3338.391477	17.173607	-0.043902	3.170266
224.218335	3330.424553	17.178611	-0.043930	3.166729
224.086509	3322.432260	17.183616	-0.043901	3.163163
224.037520	3314.463393	17.188621	-0.043886	3.159606
223.836234	3306.540702	17.193626	-0.043844	3.156060
223.766346	3298.487172	17.198631	-0.043826	3.152457
223.749862	3290.497632	17.203635	-0.043817	3.148881
223.633080	3282.466406	17.208640	-0.043790	3.145277
223.507112	3274.537168	17.213645	-0.043762	3.141715
223.644153	3266.524445	17.218650	-0.043782	3.138123
223.584892	3258.540848	17.223655	-0.043766	3.134531
223.612101	3250.553054	17.228659	-0.043766	3.130937
223.256021	3242.604682	17.233664	-0.043695	3.127339
223.354635	3234.590183	17.238669	-0.043708	3.123728
223.455999	3226.606047	17.243674	-0.043721	3.120127
223.231312	3218.662803	17.248679	-0.043675	3.116525
223.043861	3210.679658	17.253683	-0.043634	3.112902
223.046399	3202.629805	17.258688	-0.043630	3.109254
223.197464	3194.637124	17.263693	-0.043653	3.105634
223.078831	3186.700624	17.268698	-0.043626	3.102023
222.910406	3178.700905	17.273703	-0.043589	3.098377
222.831924	3170.752351	17.278707	-0.043569	3.094754
222.740996	3162.737064	17.283712	-0.043547	3.091095
222.806243	3154.734688	17.288717	-0.043554	3.087446
222.694549	3146.769200	17.293722	-0.043528	3.083801
222.524245	3138.789803	17.298727	-0.043491	3.080142
222.650543	3130.830050	17.303731	-0.043510	3.076502
222.540736	3122.751959	17.308736	-0.043484	3.072792
222.395438	3114.746415	17.313741	-0.043452	3.069109
222.440235	3106.763724	17.318746	-0.043455	3.065441
222.269167	3098.815361	17.323751	-0.043418	3.061775
222.468770	3090.839970	17.328755	-0.043450	3.058109
222.294304	3082.852268	17.333760	-0.043413	3.054415
222.281046	3074.884076	17.338765	-0.043405	3.050734
222.278067	3066.875880	17.343770	-0.043399	3.047030
221.992765	3058.907926	17.348775	-0.043341	3.043327
222.065496	3050.953156	17.353779	-0.043349	3.039642
221.982990	3042.971658	17.358784	-0.043329	3.035933
221.955430	3034.950616	17.363789	-0.043319	3.032204
221.964734	3026.958420	17.368794	-0.043315	3.028485
221.875920	3018.945413	17.373799	-0.043293	3.024748
221.744693	3011.014341	17.378803	-0.043264	3.021041
221.760992	3003.022191	17.383808	-0.043262	3.017309
221.671544	2995.055676	17.388813	-0.043240	3.013580
221.533861	2987.022840	17.393818	-0.043209	3.009812
221.434423	2979.065993	17.398823	-0.043185	3.006076
221.456795	2971.120210	17.403827	-0.043185	3.002348
221.403131	2963.124601	17.408832	-0.043169	2.998587
221.478049	2955.136059	17.413837	-0.043178	2.994832
221.230293	2947.114879	17.418842	-0.043127	2.991040
221.233153	2939.099880	17.423847	-0.043122	2.987259
221.267361	2931.148499	17.428851	-0.043124	2.983505
221.131195	2923.161274	17.433856	-0.043093	2.979721
221.147530	2915.218721	17.438861	-0.043091	2.975960
221.168817	2907.208684	17.443866	-0.043090	2.972163
220.902081	2899.220669	17.448871	-0.043035	2.968357
220.746392	2891.257376	17.453875	-0.043001	2.964563
220.806524	2883.287055	17.458880	-0.043007	2.960773
220.663613	2875.318011	17.463885	-0.042975	2.956967
220.660810	2867.327187	17.468890	-0.042969	2.953154
220.715113	2859.292849	17.473895	-0.042974	2.949318
220.750958	2851.330277	17.478899	-0.042976	2.945510
220.562117	2843.362630	17.483904	-0.042936	2.941683
220.629380	2835.375671	17.488909	-0.042943	2.937855
220.662982	2827.394956	17.493914	-0.042944	2.934023
220.427089	2819.397604	17.498919	-0.042895	2.930164
220.402849	2811.438320	17.503923	-0.042885	2.926330
220.381712	2803.445795	17.508928	-0.042876	2.922475
220.568316	2795.464314	17.513933	-0.042906	2.918630
220.297725	2787.522167	17.518938	-0.042850	2.914776
220.189971	2779.411654	17.523943	-0.042825	2.910843
220.259325	2771.470898	17.528947	-0.042833	2.906998
220.003804	2763.489721	17.533952	-0.042780	2.903109
220.117484	2755.527317	17.538957	-0.042796	2.899245
220.085907	2747.568488	17.543962	-0.042785	2.895369
219.984271	2739.566018	17.548967	-0.042761	2.891463
220.029384	2731.590063	17.553971	-0.042764	2.887573
219.876689	2723.602176	17.558976	-0.042731	2.883661
219.925016	2715.651236	17.563981	-0.042735	2.879772
219.961998	2707.685537	17.568986	-0.042736	2.875871
219.746400	2699.697870	17.573991	-0.042691	2.871939
219.659148	2691.725276	17.578995	-0.042670	2.868017
219.673653	2683.721772	17.584000	-0.042667	2.864079
219.546587	2675.769257	17.589005	-0.042638	2.860154
219.450312	2667.807186	17.594010	-0.042615	2.856220
219.319684	2659.801926	17.599015	-0.042586	2.852257
219.332378	2651.829483	17.604019	-0.042583	2.848313
219.298077	2643.825546	17.609024	-0.042572	2.844345
219.407110	2635.873118	17.614029	-0.042587	2.840405
219.120469	2627.950902	17.619034	-0.042528	2.836453
218.870437	2619.928495	17.624039	-0.042477	2.832447
219.024081	2611.910346	17.629043	-0.042500	2.828461
219.012338	2603.906058	17.634048	-0.042493	2.824466
218.869007	2595.960002	17.639053	-0.042461	2.820487
218.818922	2588.015793	17.644058	-0.042446	2.816509
218.800027	2580.003919	17.649063	-0.042438	2.812494
218.613482	2572.027757	17.654067	-0.042398	2.808480
218.785470	2564.008128	17.659072	-0.042425	2.804460
218.654629	2556.090027	17.664077	-0.042395	2.800468
218.638758	2548.123570	17.669082	-0.042387	2.796452
218.560181	2540.127611	17.674087	-0.042367	2.792412
218.782018	2532.128171	17.679091	-0.042404	2.788381
218.575509	2524.156043	17.684096	-0.042360	2.784334
218.224852	2516.237630	17.689101	-0.042290	2.780299
218.340222	2508.248922	17.694106	-0.042306	2.776251
218.035362	2500.277303	17.699111	-0.042244	2.772180
217.924749	2492.287490	17.704115	-0.042218	2.768106
217.848114	2484.312861	17.709120	-0.042199	2.764035
217.829855	2476.340118	17.714125	-0.042190	2.759962
217.960605	2468.380546	17.719130	-0.042209	2.755900
217.837556	2460.302319	17.724135	-0.042181	2.751755
217.860962	2452.326711	17.729139	-0.042181	2.747665
217.853323	2444.351447	17.734144	-0.042174	2.743568
217.786379	2436.399967	17.739149	-0.042156	2.739473
217.715552	2428.453605	17.744154	-0.042138	2.735375
217.740547	2420.435874	17.749159	-0.042138	2.731239
217.602108	2412.495580	17.754163	-0.042107	2.727127
217.383304	2404.540743	17.759168	-0.042061	2.722996
217.463044	2396.563091	17.764173	-0.042071	2.718866
217.274367	2388.623574	17.769178	-0.042030	2.714732
217.135862	2380.597253	17.774183	-0.041999	2.710550
217.198854	2372.632928	17.779187	-0.042006	2.706407
217.006826	2364.666517	17.784192	-0.041965	2.702240
217.129596	2356.685399	17.789197	-0.041983	2.698079
217.048116	2348.732772	17.794202	-0.041962	2.693913
217.006261	2340.712695	17.799207	-0.041949	2.689708
216.885964	2332.794906	17.804211	-0.041922	2.685545
217.037444	2324.799596	17.809216	-0.041945	2.681352
217.018963	2316.834339	17.814221	-0.041936	2.677158
216.965383	2308.844418	17.819226	-0.041921	2.672942
216.588264	2300.866895	17.824231	-0.041846	2.668704
216.648126	2292.890913	17.829235	-0.041852	2.664489
216.777793	2284.904279	17.834240	-0.041871	2.660267
216.669003	2276.954677	17.839245	-0.041846	2.656041
216.660162	2268.982077	17.844250	-0.041839	2.651803
216.489213	2260.992573	17.849255	-0.041802	2.647539
216.659987	2253.035230	17.854259	-0.041828	2.643308
216.415000	2245.075926	17.859264	-0.041778	2.639041
216.113999	2237.147027	17.864269	-0.041717	2.634780
216.158380	2229.148360	17.869274	-0.041720	2.630497
216.028018	2221.164510	17.874279	-0.041690	2.626204
216.106685	2213.201588	17.879283	-0.041700	2.621929
215.956075	2205.228157	17.884288	-0.041667	2.617626
215.799479	2197.273291	17.889293	-0.041632	2.613325
215.722127	2189.282493	17.894298	-0.041613	2.609004
215.727467	2181.292953	17.899303	-0.041609	2.604681
215.812010	2173.350249	17.904307	-0.041619	2.600382
215.643453	2165.399366	17.909312	-0.041583	2.596054
215.701236	2157.272919	17.914317	-0.041588	2.591639
215.841027	2149.249076	17.919322	-0.041609	2.587277
215.369019	2141.360870	17.924327	-0.041516	2.582941
215.571638	2133.403141	17.929331	-0.041549	2.578605
215.577521	2125.437845	17.934336	-0.041545	2.574245
215.283208	2117.495713	17.939341	-0.041485	2.569869
215.097040	2109.569246	17.944346	-0.041445	2.565501
215.034901	2101.606977	17.949351	-0.041428	2.561115
215.085501	2093.657972	17.954355	-0.041433	2.556737
215.076677	2085.661729	17.959360	-0.041426	2.552321
214.954929	2077.694229	17.964365	-0.041398	2.547905
215.075176	2069.711804	17.969370	-0.041415	2.543491
215.091610	2061.740928	17.974375	-0.041413	2.539067
214.787045	2053.838617	17.979379	-0.041351	2.534652
214.807761	2045.830861	17.984384	-0.041350	2.530193
214.955202	2037.848380	17.989389	-0.041372	2.525749
214.905407	2029.914890	17.994394	-0.041358	2.521311
214.879086	2021.955060	17.999399	-0.041348	2.516852
214.820352	2013.974590	18.004403	-0.041332	2.512371
214.529457	2006.010240	18.009408	-0.041273	2.507874
214.608975	1998.006228	18.014413	-0.041282	2.503374
214.521974	1990.085336	18.019418	-0.041261	2.498900
214.387985	1982.108567	18.024423	-0.041231	2.494383
214.435340	1974.132209	18.029427	-0.041234	2.489872
214.398374	1966.163605	18.034432	-0.041222	2.485350
214.268699	1958.230617	18.039437	-0.041193	2.480834
214.200997	1950.293402	18.044442	-0.041175	2.476312
213.897654	1942.330299	18.049447	-0.041114	2.471749
213.929535	1934.343815	18.054451	-0.041115	2.467189
213.878248	1926.383751	18.059456	-0.041100	2.462629
213.938517	1918.404002	18.064461	-0.041106	2.458059
213.843591	1910.468072	18.069466	-0.041083	2.453493
213.678805	1902.487846	18.074471	-0.041047	2.448888
213.865126	1894.515806	18.079475	-0.041077	2.444305
213.877504	1886.558806	18.084480	-0.041074	2.439710
213.637327	1878.647372	18.089485	-0.041024	2.435113
213.668747	1870.597916	18.094490	-0.041025	2.430447
213.492384	1862.631884	18.099495	-0.040987	2.425806
213.658099	1854.667802	18.104499	-0.041013	2.421183
213.252261	1846.766508	18.109504	-0.040932	2.416543
213.192280	1838.794158	18.114509	-0.040916	2.411880
213.207138	1830.824642	18.119514	-0.040913	2.407215
213.197750	1822.862352	18.124519	-0.040907	2.402544
212.978182	1814.953652	18.129523	-0.040861	2.397878
212.982802	1806.971223	18.134528	-0.040856	2.393178
213.040464	1798.976494	18.139533	-0.040862	2.388465
212.938797	1791.042836	18.144538	-0.040838	2.383766
212.797346	1783.102308	18.149543	-0.040806	2.379051
212.915938	1775.128495	18.154547	-0.040823	2.374328
212.703664	1767.171698	18.159552	-0.040779	2.369578
212.711668	1759.203147	18.164557	-0.040775	2.364830
212.713578	1751.261329	18.169562	-0.040770	2.360088
212.653669	1743.313321	18.174567	-0.040754	2.355327
212.714222	1735.319862	18.179571	-0.040760	2.350539
212.404537	1727.387077	18.184576	-0.040697	2.345748
212.256167	1719.443632	18.189581	-0.040665	2.340954
212.200928	1711.504930	18.194586	-0.040649	2.336160
212.056541	1703.527349	18.199591	-0.040617	2.331326
211.971884	1695.584263	18.204595	-0.040596	2.326507
212.053264	1687.613450	18.209600	-0.040606	2.321675
211.838026	1679.695070	18.214605	-0.040561	2.316841
212.150816	1671.686584	18.219610	-0.040614	2.311985
211.910745	1663.745163	18.224615	-0.040564	2.307114
211.982867	1655.792102	18.229619	-0.040573	2.302252
211.897252	1647.864232	18.234624	-0.040552	2.297381
212.008731	1639.868020	18.239629	-0.040567	2.292475
211.646006	1631.976942	18.244634	-0.040495	2.287583
211.425753	1624.043166	18.249639	-0.040448	2.282666
211.658982	1616.078595	18.254643	-0.040487	2.277758
211.579923	1608.089219	18.259648	-0.040467	2.272797
211.174382	1600.121905	18.264653	-0.040386	2.267811
211.206819	1592.178471	18.269658	-0.040387	2.262867
211.078931	1584.232663	18.274663	-0.040358	2.257896
211.016586	1576.288081	18.279667	-0.040341	2.252921
210.796810	1568.334008	18.284672	-0.040295	2.247915
210.841642	1560.385947	18.289677	-0.040299	2.242925
210.787164	1552.465686	18.294682	-0.040283	2.237933
210.819798	1544.492386	18.299687	-0.040284	2.232904
210.798016	1536.534528	18.304691	-0.040275	2.227868
210.649745	1528.607484	18.309696	-0.040242	2.222829
210.735259	1520.649476	18.314701	-0.040253	2.217780
210.725071	1512.713426	18.319706	-0.040246	2.212724
210.708568	1504.737041	18.324711	-0.040238	2.207631
210.590732	1496.834532	18.329715	-0.040211	2.202564
210.499776	1488.909523	18.334720	-0.040189	2.197474
210.395566	1480.942706	18.339725	-0.040164	2.192343
210.316999	1472.988787	18.344730	-0.040145	2.187211
210.127875	1465.056939	18.349735	-0.040104	2.182071
210.138782	1457.119593	18.354739	-0.040101	2.176934
210.231352	1449.147779	18.359744	-0.040113	2.171770
210.105272	1441.205595	18.364749	-0.040085	2.166592
210.037121	1433.295734	18.369754	-0.040067	2.161429
209.856367	1425.371737	18.374759	-0.040028	2.156233
209.778822	1417.432684	18.379763	-0.040009	2.151025
209.750952	1409.473739	18.384768	-0.039998	2.145795
209.785321	1401.524804	18.389773	-0.040000	2.140565
209.627387	1393.626630	18.394778	-0.039965	2.135338
209.614697	1385.642183	18.399783	-0.039958	2.130054
209.650192	1377.708449	18.404787	-0.039959	2.124796
209.512680	1369.798837	18.409792	-0.039928	2.119524
209.468470	1361.864181	18.414797	-0.039915	2.114231
209.498293	1353.855418	18.419802	-0.039915	2.108883
209.139907	1345.944733	18.424807	-0.039844	2.103549
208.968098	1338.051012	18.429811	-0.039806	2.098230
208.876852	1330.118955	18.434816	-0.039784	2.092881
209.031857	1322.134741	18.439821	-0.039808	2.087506
209.041551	1314.218342	18.444826	-0.039805	2.082149
208.779463	1306.320968	18.449831	-0.039751	2.076765
208.913089	1298.355844	18.454835	-0.039771	2.071359
208.778619	1290.426533	18.459840	-0.039740	2.065938
208.758230	1282.482519	18.464845	-0.039732	2.060503
208.620048	1274.595798	18.469850	-0.039701	2.055081
208.668593	1266.612582	18.474855	-0.039705	2.049597
208.696605	1258.705921	18.479859	-0.039705	2.044150
208.595833	1250.797042	18.484864	-0.039681	2.038673
208.479893	1242.877064	18.489869	-0.039654	2.033172
208.426724	1234.927164	18.494874	-0.039639	2.027642
208.257926	1227.003949	18.499879	-0.039603	2.022104
208.210731	1219.098639	18.504883	-0.039589	2.016575
208.206862	1211.146541	18.509888	-0.039583	2.011003
208.014275	1203.227330	18.514893	-0.039542	2.005418
208.112250	1195.305796	18.519898	-0.039555	1.999847
207.921619	1187.415333	18.524903	-0.039514	1.994252
207.567193	1179.503516	18.529907	-0.039443	1.988609
207.467464	1171.584830	18.534912	-0.039420	1.982971
207.615069	1163.630409	18.539917	-0.039442	1.977318
207.723150	1155.702958	18.544922	-0.039457	1.971665
207.528109	1147.777752	18.549927	-0.039416	1.965964
207.618558	1139.858096	18.554931	-0.039427	1.960281
207.452426	1131.966665	18.559936	-0.039391	1.954574
207.232043	1124.017705	18.564941	-0.039345	1.948803
207.317733	1116.084078	18.569946	-0.039356	1.943059
207.118028	1108.177731	18.574951	-0.039314	1.937287
207.148085	1100.255778	18.579955	-0.039314	1.931512
207.099724	1092.331795	18.584960	-0.039300	1.925709
206.929893	1084.449196	18.589965	-0.039263	1.919905
206.822047	1076.563172	18.594970	-0.039238	1.914088
206.648313	1068.631993	18.599975	-0.039201	1.908213
206.692973	1060.714350	18.604979	-0.039204	1.902354
206.745905	1052.791241	18.609984	-0.039209	1.896473
206.444669	1044.903357	18.614989	-0.039148	1.890561
206.463719	1036.989977	18.619994	-0.039146	1.884647
206.339538	1029.103873	18.624999	-0.039118	1.878719
206.402984	1021.174546	18.630003	-0.039125	1.872761
206.334719	1013.248760	18.635008	-0.039107	1.866771
206.345118	1005.329202	18.640013	-0.039104	1.860776
206.250116	997.452485	18.645018	-0.039081	1.854782
206.058437	989.551062	18.650023	-0.039040	1.848739
206.046053	981.647682	18.655027	-0.039033	1.842695
206.140316	973.734718	18.660032	-0.039045	1.836636
206.042888	965.836128	18.665037	-0.039022	1.830545
205.869347	957.954606	18.670042	-0.038984	1.824439
205.618928	950.095152	18.675047	-0.038933	1.818320
205.614307	942.182085	18.680051	-0.038927	1.812167
205.610551	934.272344	18.685056	-0.038921	1.805997
205.609362	926.377850	18.690061	-0.038916	1.799817
205.465901	918.509859	18.695066	-0.038884	1.793620
205.249234	910.565836	18.700071	-0.038838	1.787333
205.343325	902.657194	18.705075	-0.038851	1.781089
205.103768	894.808031	18.710080	-0.038801	1.774829
205.122663	886.886422	18.715085	-0.038800	1.768522
205.104226	879.013449	18.720090	-0.038791	1.762226
205.017736	871.137254	18.725095	-0.038770	1.755896
204.976446	863.243913	18.730099	-0.038757	1.749536
204.731438	855.391872	18.735104	-0.038706	1.743159
204.715055	847.500641	18.740109	-0.038698	1.736757
204.767753	839.606771	18.745114	-0.038703	1.730338
204.828847	831.698251	18.750119	-0.038709	1.723883
204.742363	823.858026	18.755123	-0.038688	1.717442
204.369572	816.020793	18.760128	-0.038614	1.710941
204.316138	808.120508	18.765133	-0.038599	1.704405
204.291274	800.249582	18.770138	-0.038589	1.697872
204.135091	792.371304	18.775143	-0.038555	1.691291
204.289008	784.469690	18.780147	-0.038578	1.684705
204.227335	776.621408	18.785152	-0.038562	1.678109
203.965138	768.777553	18.790157	-0.038508	1.671465
204.058452	760.885065	18.795162	-0.038520	1.664800
203.776135	753.056056	18.800167	-0.038463	1.658112
203.931178	745.158370	18.805171	-0.038486	1.651397
203.990848	737.271036	18.810176	-0.038492	1.644651
203.735021	729.467366	18.815181	-0.038440	1.637906
203.594684	721.586304	18.820186	-0.038409	1.631081
203.373870	713.719376	18.825191	-0.038362	1.624230
203.448620	705.857620	18.830195	-0.038371	1.617394
203.332225	698.003659	18.835200	-0.038345	1.610510
203.088275	690.174897	18.840205	-0.038294	1.603601
203.155169	682.323400	18.845210	-0.038301	1.596685
203.013263	674.471674	18.850215	-0.038270	1.589709
202.827682	666.642794	18.855219	-0.038230	1.582717
202.807478	658.795651	18.860224	-0.038222	1.575701
202.712577	650.949832	18.865229	-0.038199	1.568644
202.734064	643.111032	18.870234	-0.038198	1.561579
202.501280	635.302851	18.875239	-0.038149	1.554471
202.513954	627.429520	18.880243	-0.038147	1.547308
202.443129	619.598940	18.885248	-0.038128	1.540139
202.373204	611.765676	18.890253	-0.038110	1.532933
202.463134	603.915570	18.895258	-0.038122	1.525702
202.299117	596.123507	18.900263	-0.038086	1.518452
202.066565	588.320428	18.905267	-0.038038	1.511146
202.023044	580.491986	18.910272	-0.038025	1.503810
201.832620	572.692101	18.915277	-0.037985	1.496442
201.789657	564.868764	18.920282	-0.037971	1.489039
201.518907	557.077016	18.925287	-0.037916	1.481592
201.707148	549.234099	18.930291	-0.037946	1.474132
201.693845	541.368582	18.935296	-0.037938	1.466579
201.299257	533.617594	18.940301	-0.037860	1.459038
201.350214	525.805998	18.945306	-0.037864	1.451470
201.208950	518.010419	18.950311	-0.037833	1.443847
201.174684	510.228428	18.955315	-0.037822	1.436214
201.027213	502.443543	18.960320	-0.037789	1.428519
200.952166	494.643926	18.965325	-0.037770	1.420779
201.071082	486.846886	18.970330	-0.037787	1.413032
200.919365	479.058830	18.975335	-0.037754	1.405206
200.858766	471.304226	18.980339	-0.037738	1.397385
200.715625	463.524476	18.985344	-0.037706	1.389480
200.646696	455.739749	18.990349	-0.037688	1.381538
200.722147	447.962056	18.995354	-0.037697	1.373582
200.582076	440.195919	19.000359	-0.037666	1.365554
200.210956	432.499165	19.005363	-0.037592	1.357511
200.113409	424.735570	19.010368	-0.037569	1.349397
199.982212	416.975332	19.015373	-0.037540	1.341232
199.996107	409.232213	19.020378	-0.037537	1.333061
199.916284	401.472394	19.025383	-0.037517	1.324805
199.871507	393.748333	19.030387	-0.037504	1.316542
199.658060	385.909515	19.035392	-0.037459	1.308072
199.401829	378.194844	19.040397	-0.037407	1.299674
199.460309	370.453093	19.045402	-0.037412	1.291249
199.375589	362.733739	19.050407	-0.037392	1.282767
199.440754	355.013134	19.055411	-0.037399	1.274255
199.173535	347.331572	19.060416	-0.037344	1.265667
199.272160	339.605932	19.065421	-0.037358	1.257040
199.291197	331.894407	19.070426	-0.037356	1.248355
198.931177	324.252272	19.075431	-0.037284	1.239614
198.606295	316.600802	19.080435	-0.037219	1.230807
198.604464	308.889781	19.085440	-0.037213	1.221931
198.422676	301.227464	19.090445	-0.037175	1.213012
198.399771	293.545361	19.095450	-0.037165	1.204034
198.330651	285.878883	19.100455	-0.037148	1.194999
198.064621	278.250600	19.105459	-0.037093	1.185900
197.803841	270.634245	19.110464	-0.037040	1.176745
197.637205	262.984327	19.115469	-0.037004	1.167498
197.426763	255.379879	19.120474	-0.036960	1.158223
197.152464	247.722569	19.125479	-0.036904	1.148795
196.982337	240.104502	19.130483	-0.036867	1.139359
196.896489	232.478890	19.135488	-0.036846	1.129854
196.268378	224.946302	19.140493	-0.036724	1.120267
196.267988	217.328813	19.145498	-0.036719	1.110626
195.875190	209.766134	19.150503	-0.036641	1.100885
195.608010	202.204360	19.155507	-0.036587	1.091086
195.050445	194.696005	19.160512	-0.036478	1.081202
194.613761	187.160734	19.165517	-0.036392	1.071219
194.353984	179.605924	19.170522	-0.036339	1.061156
193.905072	172.095068	19.175527	-0.036250	1.051012
193.439171	164.598763	19.180531	-0.036159	1.040784
193.328731	157.057318	19.185536	-0.036133	1.030477
192.781770	149.591543	19.190541	-0.036027	1.020066
192.349824	142.128734	19.195546	-0.035941	1.009580
191.805839	134.692280	19.200551	-0.035835	0.998993
191.579418	127.177132	19.205555	-0.035788	0.988258
191.141570	119.735046	19.210560	-0.035702	0.977458
190.685150	112.303106	19.215565	-0.035612	0.966548
190.494229	104.870133	19.220570	-0.035572	0.955579
190.015977	97.474428	19.225575	-0.035478	0.944463
189.481415	90.122925	19.230579	-0.035374	0.933267
189.100699	82.753531	19.235584	-0.035298	0.921948
188.443980	75.445210	19.240589	-0.035171	0.910508
188.008676	68.110885	19.245594	-0.035085	0.898943
187.847782	60.972265	19.250599	-0.035051	0.887614