Tue Mar 23 10:17:13 2021

Number of Points = 3619
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.610077	0.017036	0.000000	-0.000018	0.743633

1.449071	-0.085643	0.005005	0.000011	0.743386
1.762693	-0.137597	0.010010	-0.000049	0.743395
1.701441	-0.132993	0.015014	-0.000039	0.743386
1.547105	-0.104595	0.020019	-0.000012	0.743390
1.498859	-0.095668	0.025024	-0.000004	0.743394
1.464510	-0.095845	0.030029	0.000001	0.743384
1.712232	-0.136168	0.035034	-0.000047	0.743394
1.485733	-0.100430	0.040038	-0.000006	0.743388
1.323663	-0.072418	0.045043	0.000023	0.743389
1.535474	-0.108938	0.050048	-0.000018	0.743393
1.669466	-0.138219	0.055053	-0.000044	0.743385
1.605997	-0.123351	0.060058	-0.000034	0.743395
1.470550	-0.105272	0.065062	-0.000010	0.743386
1.506255	-0.110980	0.070067	-0.000018	0.743390
1.550794	-0.202371	0.075072	-0.000028	0.743233
1.496014	-0.286612	0.080077	-0.000019	0.743056
1.494237	-0.282589	0.085082	-0.000020	0.743066
1.494779	-0.289580	0.090086	-0.000021	0.743055
1.560831	-0.299661	0.095091	-0.000035	0.743061
1.460853	-0.281662	0.100096	-0.000018	0.743064
1.385189	-0.275148	0.105101	-0.000005	0.743053
1.360515	-0.406706	0.110106	-0.000002	0.742797
1.342854	-0.430920	0.115110	0.000000	0.742747
1.468814	-0.454843	0.120115	-0.000025	0.742747
1.384657	-0.439656	0.125120	-0.000010	0.742750
1.348853	-0.438507	0.130125	-0.000005	0.742742
1.522033	-0.577853	0.135130	-0.000039	0.742538
1.502476	-0.635957	0.140134	-0.000036	0.742423
1.275564	-0.594454	0.145139	0.000004	0.742427
1.239552	-0.589176	0.150144	0.000010	0.742428
1.405018	-0.672554	0.155149	-0.000022	0.742327
1.329599	-0.765278	0.160154	-0.000010	0.742127
1.454076	-0.791146	0.165158	-0.000034	0.742123
1.380176	-0.778847	0.170163	-0.000022	0.742124
1.594466	-0.911802	0.175168	-0.000063	0.741945
1.342270	-0.947301	0.180173	-0.000018	0.741794
1.314749	-0.939037	0.185178	-0.000014	0.741803
0.959497	-0.895152	0.190182	0.000051	0.741769
0.923016	-1.034876	0.195187	0.000056	0.741492
1.127979	-1.070639	0.200192	0.000017	0.741496
1.144391	-1.077867	0.205197	0.000012	0.741490
1.013860	-1.175824	0.210202	0.000035	0.741261
0.888192	-1.198913	0.215206	0.000057	0.741177
0.992681	-1.218694	0.220211	0.000037	0.741177
1.104973	-1.329072	0.225216	0.000014	0.741007
0.872550	-1.339044	0.230221	0.000056	0.740911
1.249602	-1.404384	0.235226	-0.000015	0.740917
1.250843	-1.550445	0.240230	-0.000017	0.740641
1.112621	-1.558942	0.245235	0.000008	0.740580
0.787250	-1.524048	0.250240	0.000067	0.740539
0.929497	-1.698160	0.255245	0.000039	0.740256
0.941099	-1.697106	0.260250	0.000035	0.740265
0.684297	-1.745056	0.265254	0.000082	0.740088
0.753114	-1.836038	0.270259	0.000068	0.739940
0.668837	-1.819325	0.275264	0.000082	0.739946
0.561215	-1.960834	0.280269	0.000101	0.739641
0.638594	-1.971968	0.285274	0.000085	0.739648
0.512866	-2.044325	0.290278	0.000107	0.739470
0.092556	-2.052715	0.295283	0.000184	0.739313
-0.430003	-1.960032	0.300288	0.000280	0.739315
-1.302032	-1.961576	0.305293	0.000441	0.739017
-1.775411	-1.881056	0.310298	0.000527	0.739013
-1.956359	-1.851106	0.315302	0.000560	0.739011
-2.337949	-1.888423	0.320307	0.000629	0.738812
-2.610300	-1.899642	0.325312	0.000679	0.738700
-2.601567	-1.906226	0.330317	0.000676	0.738693
-2.529946	-1.915895	0.335322	0.000661	0.738702
-3.416750	-1.914831	0.340326	0.000825	0.738404
-3.650728	-1.875572	0.345331	0.000867	0.738402
-3.438607	-1.913032	0.350336	0.000826	0.738405
-3.953610	-1.827138	0.355341	0.000920	0.738396
-3.875331	-1.973620	0.360346	0.000905	0.738145
-4.643417	-1.879069	0.365350	0.001046	0.738066
-4.692978	-1.871625	0.370355	0.001054	0.738066
-4.707419	-1.867417	0.375360	0.001055	0.738072
-4.676456	-1.896327	0.380365	0.001048	0.738030
-5.364314	-1.917642	0.385370	0.001175	0.737756
-5.660551	-1.869300	0.390374	0.001229	0.737751
-5.615890	-1.879302	0.395379	0.001219	0.737749
-5.318489	-1.930141	0.400384	0.001162	0.737756
-5.849304	-1.843094	0.405389	0.001260	0.737744
-6.030172	-1.942966	0.410394	0.001292	0.737493
-6.706049	-1.858187	0.415398	0.001416	0.737428
-6.731528	-1.855025	0.420403	0.001420	0.737427
-6.685128	-1.862411	0.425408	0.001410	0.737432
-6.894980	-1.829794	0.430413	0.001447	0.737425
-6.814259	-1.840399	0.435418	0.001431	0.737435
-7.129790	-1.887679	0.440422	0.001488	0.737239
-7.962916	-1.796198	0.445427	0.001642	0.737132
-7.547341	-1.870453	0.450432	0.001563	0.737134
-7.684464	-1.852391	0.455437	0.001587	0.737125
-7.803898	-1.827608	0.460442	0.001608	0.737134
-7.871873	-1.819934	0.465446	0.001619	0.737128
-7.833599	-1.827988	0.470451	0.001611	0.737128
-8.114500	-1.911619	0.475456	0.001662	0.736874
-8.753009	-1.836047	0.480461	0.001779	0.736804
-8.445365	-1.886565	0.485466	0.001721	0.736814
-8.523725	-1.879031	0.490470	0.001734	0.736804
-8.990228	-1.796872	0.495475	0.001819	0.736805
-8.564982	-1.871308	0.500480	0.001739	0.736810
-8.720706	-1.847825	0.505485	0.001766	0.736805
-9.223731	-1.897124	0.510490	0.001859	0.736540
-9.605894	-1.847406	0.515494	0.001928	0.736508
-9.717456	-1.829787	0.520499	0.001948	0.736506
-9.462153	-1.872705	0.525504	0.001899	0.736513
-9.788413	-1.820677	0.530509	0.001958	0.736504
-9.643538	-1.843835	0.535514	0.001930	0.736512
-9.486824	-1.877130	0.540518	0.001899	0.736504
-10.055285	-1.897093	0.545523	0.002004	0.736274
-10.569996	-1.843136	0.550528	0.002098	0.736204
-10.541472	-1.854484	0.555533	0.002091	0.736194
-10.530799	-1.852967	0.560538	0.002088	0.736204
-10.631745	-1.839789	0.565542	0.002105	0.736197
-10.608352	-1.846616	0.570547	0.002100	0.736194
-10.437223	-1.873472	0.575552	0.002067	0.736204
-10.513727	-1.924404	0.580557	0.002079	0.736082
-11.294889	-1.862002	0.585562	0.002223	0.735937
-11.020013	-1.914283	0.590566	0.002171	0.735933
-11.520927	-1.827702	0.595571	0.002263	0.735931
-11.301020	-1.865668	0.600576	0.002220	0.735936
-11.481762	-1.838784	0.605581	0.002253	0.735928
-11.478374	-1.836540	0.610586	0.002251	0.735936
-11.352485	-1.952416	0.615590	0.002226	0.735759
-12.406468	-1.851301	0.620595	0.002421	0.735595
-12.326602	-1.864403	0.625600	0.002404	0.735600
-12.826506	-1.780348	0.630605	0.002496	0.735593
-12.567390	-1.823831	0.635610	0.002446	0.735601
-12.336829	-1.868474	0.640614	0.002402	0.735596
-12.795096	-1.787449	0.645619	0.002486	0.735598
-12.434809	-1.849492	0.650624	0.002418	0.735604
-12.684970	-1.949879	0.655629	0.002463	0.735328
-13.450891	-1.834019	0.660634	0.002604	0.735291
-13.745765	-1.787560	0.665638	0.002657	0.735282
-13.436869	-1.841519	0.670643	0.002599	0.735286
-13.123705	-1.897371	0.675648	0.002539	0.735289
-13.460710	-1.841556	0.680653	0.002600	0.735283
-13.460976	-1.840326	0.685658	0.002599	0.735288
-13.219718	-1.938985	0.690662	0.002553	0.735183
-14.411130	-1.842654	0.695667	0.002773	0.734963
-13.866391	-1.938076	0.700672	0.002670	0.734968
-14.271741	-1.871033	0.705677	0.002744	0.734961
-14.687687	-1.793971	0.710682	0.002820	0.734970
-14.390100	-1.850939	0.715686	0.002764	0.734964
-14.465292	-1.840028	0.720691	0.002776	0.734962
-14.495840	-1.833414	0.725696	0.002780	0.734967
-14.855152	-1.871364	0.730701	0.002846	0.734773
-15.409208	-1.829216	0.735706	0.002948	0.734667
-14.924809	-1.920301	0.740710	0.002856	0.734660
-15.193536	-1.874319	0.745715	0.002905	0.734659
-15.713347	-1.777205	0.750720	0.003000	0.734671
-15.364591	-1.846633	0.755725	0.002934	0.734659
-15.420064	-1.835020	0.760730	0.002943	0.734665
-15.732837	-1.782377	0.765734	0.003000	0.734662
-15.919124	-1.881674	0.770739	0.003033	0.734409
-16.115774	-1.882158	0.775744	0.003068	0.734343
-16.315823	-1.849846	0.780749	0.003104	0.734339
-16.271176	-1.856042	0.785754	0.003094	0.734345
-16.498287	-1.818472	0.790758	0.003135	0.734342
-16.786118	-1.770870	0.795763	0.003187	0.734338
-16.253219	-1.863991	0.800768	0.003087	0.734344
-16.287018	-1.865212	0.805773	0.003092	0.734332
-17.059977	-1.875538	0.810778	0.003234	0.734049
-17.478206	-1.811328	0.815782	0.003311	0.734032
-17.494143	-1.810065	0.820787	0.003312	0.734032
-17.078838	-1.879847	0.825792	0.003234	0.734042
-17.562830	-1.798282	0.830797	0.003322	0.734036
-17.513131	-1.805136	0.835802	0.003312	0.734043
-16.905727	-1.919233	0.840806	0.003197	0.734033
-17.510200	-1.825938	0.845811	0.003308	0.734008
-18.196015	-1.850763	0.850816	0.003435	0.733728
-18.069294	-1.880734	0.855821	0.003410	0.733716
-18.210570	-1.851600	0.860826	0.003435	0.733726
-18.450573	-1.813147	0.865830	0.003478	0.733720
-18.530399	-1.803873	0.870835	0.003491	0.733713
-18.310808	-1.837675	0.875840	0.003449	0.733726
-18.560722	-1.798995	0.880845	0.003494	0.733718
-18.364070	-1.859989	0.885850	0.003456	0.733670
-19.012355	-1.877807	0.890854	0.003576	0.733415
-19.284486	-1.834041	0.895859	0.003625	0.733409
-19.255052	-1.835073	0.900864	0.003618	0.733420
-19.220450	-1.848413	0.905869	0.003610	0.733408
-19.117309	-1.861061	0.910874	0.003590	0.733422
-19.706261	-1.762030	0.915878	0.003698	0.733413
-19.612679	-1.782105	0.920883	0.003679	0.733409
-19.099131	-1.935195	0.925888	0.003582	0.733292
-20.769917	-1.754545	0.930893	0.003892	0.733070
-20.386501	-1.820162	0.935898	0.003819	0.733077
-20.071470	-1.878135	0.940902	0.003759	0.733076
-20.408165	-1.822841	0.945907	0.003820	0.733070
-20.370637	-1.826163	0.950912	0.003812	0.733079
-20.317048	-1.840536	0.955917	0.003800	0.733072
-20.279649	-1.842624	0.960922	0.003792	0.733083
-20.410393	-1.891008	0.965926	0.003815	0.732947
-21.531499	-1.792662	0.970931	0.004022	0.732755
-20.997531	-1.884498	0.975936	0.003922	0.732763
-21.272990	-1.843322	0.980941	0.003971	0.732751
-21.492219	-1.802022	0.985946	0.004011	0.732758
-21.007171	-1.888787	0.990950	0.003919	0.732759
-21.345496	-1.830941	0.995955	0.003981	0.732757
-21.225101	-1.851830	1.000960	0.003957	0.732761
-21.506093	-1.926175	1.005965	0.004008	0.732523
-22.337942	-1.821471	1.010970	0.004161	0.732442
-22.526857	-1.789073	1.015974	0.004195	0.732442
-22.128411	-1.865718	1.020979	0.004120	0.732433
-21.928451	-1.897980	1.025984	0.004081	0.732442
-22.188563	-1.858079	1.030989	0.004128	0.732433
-22.348585	-1.826666	1.035994	0.004156	0.732441
-22.305576	-1.837380	1.040998	0.004147	0.732438
-22.964474	-1.874675	1.046003	0.004268	0.732141
-22.907726	-1.883116	1.051008	0.004256	0.732147
-23.369965	-1.804875	1.056013	0.004341	0.732142
-22.842297	-1.898743	1.061018	0.004241	0.732144
-23.089366	-1.856120	1.066022	0.004286	0.732144
-23.462175	-1.793506	1.071027	0.004354	0.732140
-23.224306	-1.833966	1.076032	0.004308	0.732146
-23.226740	-1.902218	1.081037	0.004307	0.732015
-24.591639	-1.760516	1.086042	0.004560	0.731822
-23.967121	-1.876129	1.091046	0.004443	0.731816
-23.884182	-1.893583	1.096051	0.004426	0.731813
-23.877460	-1.892522	1.101056	0.004423	0.731820
-24.101453	-1.857790	1.106061	0.004463	0.731813
-24.073550	-1.859328	1.111066	0.004457	0.731822
-24.099148	-1.858722	1.116070	0.004460	0.731817
-24.746006	-1.887384	1.121075	0.004579	0.731541
-25.186207	-1.821960	1.126080	0.004660	0.731519
-25.585245	-1.756004	1.131085	0.004733	0.731512
-25.232189	-1.817041	1.136090	0.004666	0.731518
-25.007392	-1.858886	1.141094	0.004622	0.731517
-25.095957	-1.846432	1.146099	0.004637	0.731513
-24.999368	-1.861199	1.151104	0.004618	0.731520
-25.099488	-1.849227	1.156109	0.004635	0.731511
-25.313764	-1.959695	1.161114	0.004674	0.731226
-25.777623	-1.890216	1.166118	0.004759	0.731203
-26.253651	-1.807661	1.171123	0.004846	0.731202
-25.865772	-1.874172	1.176128	0.004772	0.731209
-25.695042	-1.909458	1.181133	0.004739	0.731202
-26.134380	-1.829486	1.186138	0.004820	0.731208
-26.253729	-1.811997	1.191142	0.004840	0.731203
-26.308729	-1.899061	1.196147	0.004849	0.731018
-27.144255	-1.803133	1.201152	0.005003	0.730919
-27.149477	-1.807195	1.206157	0.005003	0.730911
-26.886440	-1.851861	1.211162	0.004953	0.730918
-26.948241	-1.843885	1.216166	0.004963	0.730915
-27.111792	-1.819134	1.221171	0.004992	0.730909
-26.956779	-1.843857	1.226176	0.004962	0.730917
-27.007949	-1.839905	1.231181	0.004970	0.730910
-27.564548	-1.887891	1.236186	0.005072	0.730627
-28.142688	-1.806995	1.241190	0.005178	0.730587
-28.100988	-1.818760	1.246195	0.005169	0.730581
-27.872437	-1.857252	1.251200	0.005125	0.730588
-28.388937	-1.771515	1.256205	0.005220	0.730579
-28.151511	-1.812672	1.261210	0.005174	0.730583
-27.848571	-1.869588	1.266214	0.005117	0.730580
-28.280054	-1.794753	1.271219	0.005195	0.730579
-28.350770	-1.903422	1.276224	0.005207	0.730346
-28.913841	-1.846505	1.281229	0.005311	0.730265
-28.973691	-1.833487	1.286234	0.005320	0.730272
-29.188883	-1.801072	1.291238	0.005359	0.730263
-29.364856	-1.770650	1.296243	0.005390	0.730264
-29.183049	-1.799904	1.301248	0.005355	0.730273
-29.101059	-1.820042	1.306253	0.005339	0.730264
-29.167469	-1.806178	1.311258	0.005350	0.730271
-29.331183	-1.894992	1.316262	0.005379	0.730044
-30.371146	-1.758148	1.321267	0.005571	0.729953
-30.004759	-1.821893	1.326272	0.005501	0.729959
-29.790422	-1.867425	1.331277	0.005460	0.729947
-30.188314	-1.793138	1.336282	0.005533	0.729956
-30.072495	-1.817525	1.341286	0.005510	0.729952
-29.775311	-1.874664	1.346291	0.005453	0.729946
-29.728794	-1.889293	1.351296	0.005443	0.729936
-30.883743	-1.832494	1.356301	0.005657	0.729650
-30.805402	-1.844147	1.361306	0.005641	0.729657
-30.790330	-1.850206	1.366310	0.005636	0.729653
-30.955931	-1.824842	1.371315	0.005666	0.729648
-30.823023	-1.843754	1.376320	0.005640	0.729659
-30.887153	-1.839296	1.381325	0.005650	0.729648
-30.785175	-1.856320	1.386330	0.005630	0.729653
-31.003119	-1.914539	1.391334	0.005669	0.729467
-32.179204	-1.779003	1.396339	0.005887	0.729327
-31.942172	-1.820139	1.401344	0.005841	0.729331
-32.060725	-1.803546	1.406349	0.005862	0.729325
-31.872673	-1.833879	1.411354	0.005825	0.729334
-31.898968	-1.832497	1.416358	0.005829	0.729330
-32.081119	-1.803463	1.421363	0.005861	0.729326
-31.938437	-1.825763	1.426368	0.005834	0.729334
-32.275781	-1.874091	1.431373	0.005895	0.729126
-33.218572	-1.763251	1.436378	0.006069	0.729018
-32.829582	-1.832712	1.441382	0.005995	0.729020
-32.480769	-1.897151	1.446387	0.005929	0.729018
-32.694960	-1.856034	1.451392	0.005967	0.729027
-33.347582	-1.749786	1.456397	0.006088	0.729010
-33.192878	-1.775874	1.461402	0.006057	0.729016
-32.851732	-1.836300	1.466406	0.005992	0.729019
-33.144294	-1.920749	1.471411	0.006046	0.728756
-33.771804	-1.839142	1.476416	0.006161	0.728700
-34.073914	-1.789602	1.481421	0.006216	0.728694
-33.804228	-1.835670	1.486426	0.006164	0.728701
-33.798166	-1.838519	1.491430	0.006162	0.728700
-34.030796	-1.800781	1.496435	0.006204	0.728695
-33.725180	-1.852039	1.501440	0.006145	0.728704
-34.116045	-1.806641	1.506445	0.006217	0.728659
-34.702043	-1.838283	1.511450	0.006325	0.728397
-34.599323	-1.858933	1.516454	0.006304	0.728395
-35.222582	-1.751201	1.521459	0.006419	0.728392
-34.990472	-1.789383	1.526464	0.006374	0.728401
-34.746799	-1.838683	1.531469	0.006327	0.728392
-34.956746	-1.799686	1.536474	0.006365	0.728397
-34.959061	-1.802488	1.541478	0.006364	0.728394
-34.752536	-1.881342	1.546483	0.006324	0.728314
-35.443243	-1.885827	1.551488	0.006451	0.728069
-35.788488	-1.831531	1.556493	0.006514	0.728057
-36.060292	-1.780286	1.561498	0.006563	0.728066
-35.883386	-1.814377	1.566502	0.006529	0.728063
-35.681574	-1.853903	1.571507	0.006490	0.728059
-36.038706	-1.787553	1.576512	0.006555	0.728067
-35.841523	-1.828259	1.581517	0.006517	0.728058
-35.717520	-1.943418	1.586522	0.006493	0.727880
-36.683217	-1.835597	1.591526	0.006671	0.727758
-36.912076	-1.800127	1.596531	0.006712	0.727750
-36.554441	-1.861493	1.601536	0.006644	0.727757
-36.959975	-1.794262	1.606541	0.006718	0.727750
-37.060982	-1.774893	1.611546	0.006736	0.727755
-36.637036	-1.853987	1.616550	0.006656	0.727751
-36.975429	-1.796301	1.621555	0.006717	0.727748
-37.217438	-1.886651	1.626560	0.006761	0.727491
-37.795568	-1.814008	1.631565	0.006867	0.727435
-37.747387	-1.821309	1.636570	0.006857	0.727440
-37.659955	-1.840760	1.641574	0.006839	0.727435
-37.972378	-1.786972	1.646579	0.006896	0.727434
-37.667842	-1.839372	1.651584	0.006838	0.727440
-37.782565	-1.823369	1.656589	0.006858	0.727434
-38.022676	-1.784131	1.661594	0.006901	0.727430
-38.210300	-1.899147	1.666598	0.006935	0.727143
-38.485023	-1.852027	1.671603	0.006984	0.727142
-38.773801	-1.798803	1.676608	0.007037	0.727148
-38.725546	-1.814083	1.681613	0.007026	0.727138
-38.559933	-1.841283	1.686618	0.006994	0.727145
-38.509344	-1.851855	1.691622	0.006983	0.727144
-38.744535	-1.812771	1.696627	0.007026	0.727141
-38.579273	-1.954037	1.701632	0.006994	0.726926
-39.668748	-1.815491	1.706637	0.007195	0.726820
-39.737089	-1.803538	1.711642	0.007206	0.726823
-39.162862	-1.908059	1.716646	0.007098	0.726821
-39.589030	-1.836106	1.721651	0.007176	0.726816
-39.731073	-1.808596	1.726656	0.007201	0.726823
-39.777137	-1.805608	1.731661	0.007208	0.726815
-39.774120	-1.842437	1.736666	0.007206	0.726747
-40.623875	-1.812758	1.741670	0.007363	0.726512
-40.648388	-1.813483	1.746675	0.007366	0.726505
-40.623797	-1.814591	1.751680	0.007360	0.726514
-40.619572	-1.820431	1.756685	0.007358	0.726507
-40.422744	-1.853231	1.761690	0.007320	0.726514
-40.411445	-1.856611	1.766694	0.007317	0.726513
-40.690739	-1.811594	1.771699	0.007367	0.726507
-40.773682	-1.882243	1.776704	0.007381	0.726343
-42.017782	-1.738186	1.781709	0.007612	0.726194
-41.558162	-1.818677	1.786714	0.007525	0.726199
-41.319965	-1.863958	1.791718	0.007479	0.726196
-41.906402	-1.763875	1.796723	0.007587	0.726191
-41.519489	-1.827630	1.801728	0.007513	0.726203
-41.478576	-1.841077	1.806733	0.007504	0.726194
-41.662028	-1.805880	1.811738	0.007537	0.726201
-41.536948	-1.908919	1.816742	0.007512	0.726046
-42.551815	-1.795954	1.821747	0.007700	0.725917
-42.188411	-1.856807	1.826752	0.007631	0.725927
-42.391152	-1.827407	1.831757	0.007667	0.725916
-42.255394	-1.849422	1.836762	0.007641	0.725923
-42.261074	-1.850061	1.841766	0.007640	0.725922
-42.599947	-1.792677	1.846771	0.007702	0.725919
-42.273156	-1.928549	1.851776	0.007640	0.725770
-43.421613	-1.818853	1.856781	0.007852	0.725588
-43.159826	-1.863821	1.861786	0.007802	0.725593
-43.058185	-1.883040	1.866790	0.007782	0.725594
-43.328763	-1.838529	1.871795	0.007831	0.725589
-43.040666	-1.887420	1.876800	0.007776	0.725596
-43.450980	-1.820434	1.881805	0.007851	0.725587
-43.396210	-1.894281	1.886810	0.007839	0.725465
-44.028374	-1.876232	1.891814	0.007955	0.725282
-44.269202	-1.837013	1.896819	0.007999	0.725278
-44.349029	-1.817269	1.901824	0.008012	0.725291
-44.443469	-1.806420	1.906829	0.008028	0.725282
-44.302846	-1.830064	1.911834	0.008001	0.725288
-44.418357	-1.809677	1.916838	0.008021	0.725290
-44.408878	-1.817922	1.921843	0.008018	0.725280
-44.433184	-1.931779	1.926848	0.008021	0.725051
-45.353895	-1.811168	1.931853	0.008191	0.724969
-45.248514	-1.830456	1.936858	0.008170	0.724971
-45.117901	-1.856031	1.941862	0.008144	0.724969
-45.756553	-1.744167	1.946867	0.008262	0.724968
-45.389143	-1.804507	1.951872	0.008192	0.724980
-45.090108	-1.866522	1.956877	0.008135	0.724966
-45.417783	-1.807096	1.961882	0.008195	0.724970
-46.022544	-1.853199	1.966886	0.008306	0.724672
-46.077747	-1.851562	1.971891	0.008315	0.724659
-46.138145	-1.834604	1.976896	0.008325	0.724673
-46.378767	-1.798848	1.981901	0.008368	0.724662
-46.311064	-1.809317	1.986906	0.008354	0.724668
-45.997390	-1.866797	1.991910	0.008294	0.724667
-46.207698	-1.832209	1.996915	0.008332	0.724664
-46.774594	-1.852742	2.001920	0.008436	0.724429

-47.123399	-1.845400	2.011917	0.008498	0.724327
-47.251610	-1.825434	2.021914	0.008519	0.724327
-47.425718	-1.799534	2.031910	0.008549	0.724322
-47.018886	-1.870773	2.041907	0.008470	0.724330
-47.079843	-1.861741	2.051904	0.008479	0.724331
-47.171829	-1.848263	2.061901	0.008493	0.724331
-47.220595	-1.843476	2.071898	0.008500	0.724328
-47.574426	-1.786105	2.081894	0.008563	0.724323
-47.293311	-1.797927	2.091891	0.008508	0.724403
-46.576909	-1.793318	2.101888	0.008371	0.724666
-46.153995	-1.869851	2.111885	0.008290	0.724669
-46.455213	-1.819971	2.121882	0.008343	0.724667
-46.495286	-1.816093	2.131878	0.008348	0.724666
-46.301665	-1.853132	2.141875	0.008309	0.724666
-46.522516	-1.814721	2.151872	0.008347	0.724669
-45.857334	-1.795787	2.161869	0.008221	0.724943
-45.888308	-1.777150	2.171866	0.008224	0.724974
-45.744922	-1.806965	2.181862	0.008194	0.724971
-45.632686	-1.829717	2.191859	0.008171	0.724971
-45.196221	-1.794908	2.201856	0.008087	0.725196
-44.869488	-1.809918	2.211853	0.008023	0.725286
-44.968997	-1.794703	2.221850	0.008039	0.725286
-44.871542	-1.816103	2.231846	0.008018	0.725283
-44.115062	-1.806852	2.241843	0.007874	0.725570
-44.231784	-1.774579	2.251840	0.007893	0.725597
-44.023633	-1.813761	2.261837	0.007852	0.725598
-44.130161	-1.734916	2.271834	0.007869	0.725721
-43.164129	-1.804910	2.281830	0.007686	0.725925
-43.096869	-1.818976	2.291827	0.007671	0.725926
-43.193151	-1.803576	2.301824	0.007686	0.725928
-42.710068	-1.786662	2.311821	0.007593	0.726134
-42.506386	-1.790832	2.321818	0.007552	0.726202
-42.463977	-1.801876	2.331814	0.007542	0.726200
-42.381334	-1.761287	2.341811	0.007524	0.726313
-41.511517	-1.814540	2.351808	0.007359	0.726517
-41.482041	-1.823202	2.361805	0.007351	0.726515
-41.610660	-1.803848	2.371802	0.007372	0.726514
-41.035403	-1.758107	2.381798	0.007262	0.726808
-40.732085	-1.806410	2.391795	0.007203	0.726824
-40.621718	-1.828667	2.401792	0.007179	0.726824
-40.479439	-1.757692	2.411789	0.007150	0.727017
-40.048831	-1.769540	2.421786	0.007067	0.727149
-39.844003	-1.810731	2.431782	0.007026	0.727145
-39.674334	-1.813443	2.441779	0.006992	0.727203
-39.155533	-1.785243	2.451776	0.006892	0.727444
-38.785440	-1.854681	2.461773	0.006821	0.727442
-39.253357	-1.773306	2.471770	0.006905	0.727443
-38.479333	-1.782940	2.481766	0.006758	0.727698
-38.424326	-1.765945	2.491763	0.006745	0.727755
-38.025268	-1.839413	2.501760	0.006668	0.727756
-38.134722	-1.744890	2.511757	0.006686	0.727907
-37.385710	-1.798299	2.521754	0.006543	0.728068
-37.538862	-1.774704	2.531750	0.006569	0.728066
-37.488543	-1.745180	2.541747	0.006557	0.728146
-36.488452	-1.795304	2.551744	0.006368	0.728400
-36.343855	-1.823569	2.561741	0.006338	0.728400
-36.818226	-1.741933	2.571738	0.006424	0.728400
-35.823976	-1.781247	2.581734	0.006236	0.728673
-35.832840	-1.767504	2.591731	0.006235	0.728702
-35.553134	-1.818444	2.601728	0.006180	0.728705
-35.342791	-1.787429	2.611725	0.006138	0.728843
-34.548445	-1.837290	2.621722	0.005987	0.729026
-34.814303	-1.793042	2.631718	0.006034	0.729026
-34.842690	-1.791811	2.641715	0.006037	0.729023
-34.177487	-1.770392	2.651712	0.005910	0.729300
-33.956135	-1.793096	2.661709	0.005866	0.729338
-33.986842	-1.790930	2.671706	0.005869	0.729337
-33.498373	-1.791563	2.681702	0.005775	0.729509
-33.222357	-1.766316	2.691699	0.005721	0.729659
-33.078056	-1.793842	2.701696	0.005691	0.729661
-33.049298	-1.784560	2.711693	0.005683	0.729694
-32.567486	-1.736202	2.721690	0.005591	0.729959
-32.125309	-1.819743	2.731686	0.005506	0.729955
-32.360622	-1.781255	2.741683	0.005547	0.729954
-31.499030	-1.814422	2.751680	0.005383	0.730192
-31.596552	-1.756856	2.761677	0.005399	0.730275
-31.505898	-1.775519	2.771674	0.005379	0.730276
-31.320279	-1.741148	2.781670	0.005342	0.730412
-30.546364	-1.794153	2.791667	0.005195	0.730581
-30.444894	-1.811720	2.801664	0.005173	0.730587
-30.567508	-1.792157	2.811661	0.005193	0.730588
-29.928994	-1.739424	2.821658	0.005072	0.730916
-29.849931	-1.755782	2.831654	0.005054	0.730917
-29.877230	-1.752452	2.841651	0.005056	0.730919
-29.170958	-1.772275	2.851648	0.004922	0.731129
-28.956786	-1.772887	2.861645	0.004879	0.731207
-28.692922	-1.822122	2.871642	0.004828	0.731208
-28.881472	-1.748985	2.881638	0.004860	0.731290
-28.082075	-1.775757	2.891635	0.004708	0.731518
-27.772576	-1.832182	2.901632	0.004648	0.731521
-28.110389	-1.773044	2.911629	0.004708	0.731524
-27.257324	-1.796169	2.921626	0.004546	0.731779
-27.170784	-1.790618	2.931622	0.004527	0.731824
-27.312611	-1.768163	2.941619	0.004551	0.731824
-27.161673	-1.719956	2.951616	0.004520	0.731975
-26.215272	-1.803070	2.961613	0.004341	0.732145
-26.434567	-1.767117	2.971610	0.004379	0.732144
-26.562624	-1.711469	2.981606	0.004400	0.732213
-25.535081	-1.779507	2.991603	0.004206	0.732440
-25.546335	-1.778948	3.001600	0.004206	0.732442
-25.818134	-1.732404	3.011597	0.004253	0.732444
-24.794634	-1.754800	3.021594	0.004060	0.732758
-24.684803	-1.776184	3.031590	0.004037	0.732760
-24.776669	-1.761163	3.041587	0.004051	0.732762
-24.434223	-1.729460	3.051584	0.003985	0.732947
-23.859154	-1.766595	3.061581	0.003875	0.733078
-23.751201	-1.788452	3.071578	0.003852	0.733078
-23.829609	-1.738962	3.081574	0.003864	0.733152
-22.646586	-1.817543	3.091571	0.003641	0.733412
-22.863584	-1.782043	3.101568	0.003678	0.733411
-22.630026	-1.823492	3.111565	0.003632	0.733416
-22.559138	-1.761956	3.121562	0.003616	0.733564
-21.855159	-1.809456	3.131558	0.003482	0.733720
-21.753954	-1.828493	3.141555	0.003461	0.733723
-21.721428	-1.837863	3.151552	0.003452	0.733721
-21.424477	-1.783120	3.161549	0.003394	0.733934
-21.155242	-1.777206	3.171546	0.003341	0.734043
-21.407911	-1.735525	3.181542	0.003385	0.734042
-20.842845	-1.778538	3.191539	0.003277	0.734158
-19.996570	-1.835846	3.201536	0.003117	0.734343
-20.066017	-1.826431	3.211533	0.003127	0.734342
-20.008089	-1.839429	3.221530	0.003113	0.734342
-19.603595	-1.808533	3.231526	0.003035	0.734546
-19.365244	-1.793672	3.241523	0.002988	0.734661
-19.286499	-1.810169	3.251520	0.002971	0.734662
-19.117070	-1.818206	3.261517	0.002936	0.734710
-18.496467	-1.798091	3.271514	0.002818	0.734966
-18.257253	-1.842156	3.281510	0.002771	0.734969
-18.165595	-1.862368	3.291507	0.002751	0.734966
-18.168383	-1.784962	3.301504	0.002748	0.735120
-17.163683	-1.878899	3.311501	0.002559	0.735288
-17.477678	-1.825221	3.321498	0.002614	0.735289
-17.462247	-1.831309	3.331494	0.002609	0.735288
-16.674471	-1.828196	3.341491	0.002459	0.735569
-16.445443	-1.856046	3.351488	0.002414	0.735599
-16.420040	-1.862122	3.361485	0.002406	0.735601
-16.497360	-1.811594	3.371482	0.002418	0.735677
-15.592021	-1.842413	3.381478	0.002247	0.735933
-15.488892	-1.862231	3.391475	0.002225	0.735935
-15.762976	-1.815855	3.401472	0.002273	0.735935
-15.179307	-1.827576	3.411469	0.002161	0.736118
-15.064976	-1.807287	3.421466	0.002137	0.736201
-14.909244	-1.838610	3.431462	0.002105	0.736199
-14.787590	-1.798016	3.441459	0.002080	0.736324
-13.911973	-1.861153	3.451456	0.001914	0.736507
-13.910539	-1.861138	3.461453	0.001911	0.736513
-13.938002	-1.860126	3.471450	0.001914	0.736511
-13.288986	-1.838203	3.481446	0.001790	0.736780
-13.393528	-1.806378	3.491443	0.001807	0.736811
-13.102715	-1.861113	3.501440	0.001750	0.736810
-12.840684	-1.816893	3.511437	0.001698	0.736990
-12.463638	-1.812412	3.521434	0.001625	0.737132
-12.185571	-1.865042	3.531430	0.001571	0.737131
-12.315021	-1.815160	3.541427	0.001592	0.737188
-11.485348	-1.839376	3.551424	0.001435	0.737430
-11.558425	-1.827449	3.561421	0.001445	0.737433
-11.271889	-1.880974	3.571418	0.001389	0.737433
-10.816719	-1.840378	3.581414	0.001302	0.737672
-10.515276	-1.853669	3.591411	0.001243	0.737754
-10.548122	-1.849423	3.601408	0.001246	0.737756
-10.442403	-1.834253	3.611405	0.001224	0.737827
-9.788343	-1.825695	3.621402	0.001099	0.738072
-9.568100	-1.865721	3.631398	0.001055	0.738075
-9.940883	-1.804610	3.641395	0.001122	0.738070
-8.933081	-1.835980	3.651392	0.000932	0.738359
-8.834747	-1.828220	3.661389	0.000910	0.738413
-8.820686	-1.836184	3.671386	0.000905	0.738407
-8.900033	-1.766972	3.681382	0.000917	0.738518
-8.219724	-1.793144	3.691379	0.000788	0.738705
-7.950879	-1.842500	3.701376	0.000735	0.738707
-8.003399	-1.816786	3.711373	0.000742	0.738744
-7.111699	-1.835022	3.721370	0.000573	0.739018
-7.209010	-1.822003	3.731366	0.000588	0.739015
-7.277858	-1.811599	3.741363	0.000598	0.739016
-6.649723	-1.818552	3.751360	0.000479	0.739222
-6.297158	-1.831778	3.761357	0.000410	0.739322
-6.149439	-1.862490	3.771354	0.000380	0.739318
-6.223630	-1.827157	3.781350	0.000391	0.739366
-5.598055	-1.794759	3.791347	0.000272	0.739646
-5.295577	-1.851110	3.801344	0.000213	0.739646
-5.446005	-1.825793	3.811341	0.000238	0.739649
-5.127135	-1.769823	3.821338	0.000176	0.739869
-4.749742	-1.800678	3.831334	0.000103	0.739944
-4.753390	-1.803499	3.841331	0.000101	0.739942
-4.391389	-1.776051	3.851328	0.000030	0.740123
-3.968969	-1.778922	3.861325	-0.000051	0.740267
-3.859850	-1.801220	3.871322	-0.000074	0.740266
-3.718567	-1.779496	3.881318	-0.000103	0.740361
-3.330222	-1.737310	3.891315	-0.000178	0.740579
-3.071052	-1.785304	3.901312	-0.000229	0.740580
-3.143369	-1.749443	3.911309	-0.000219	0.740629
-2.867713	-1.650355	3.921306	-0.000273	0.740917
-2.813299	-1.662599	3.931302	-0.000286	0.740918
-2.759181	-1.616830	3.941299	-0.000299	0.741029
-2.000181	-1.669910	3.951296	-0.000443	0.741190
-2.097101	-1.655251	3.961293	-0.000428	0.741190
-1.924101	-1.579268	3.971290	-0.000463	0.741399
-1.830970	-1.546325	3.981286	-0.000483	0.741499
-1.702070	-1.547758	3.991283	-0.000509	0.741545
-1.678076	-1.420433	4.001280	-0.000517	0.741802
-1.398940	-1.472094	4.011277	-0.000572	0.741803
-1.326457	-1.329556	4.021274	-0.000588	0.742104
-1.053123	-1.368679	4.031270	-0.000642	0.742128
-1.091741	-1.240642	4.041267	-0.000637	0.742364
-0.955544	-1.235600	4.051264	-0.000665	0.742425
-0.741222	-1.133382	4.061261	-0.000708	0.742698
-0.863195	-1.084646	4.071258	-0.000688	0.742754
-0.665173	-0.964627	4.081254	-0.000728	0.743055
-0.597878	-0.922954	4.091251	-0.000743	0.743163
-0.535729	-0.820118	4.101248	-0.000758	0.743385
-0.380192	-0.735077	4.111245	-0.000789	0.743604
-0.282761	-0.682798	4.121242	-0.000810	0.743742
-0.261601	-0.553252	4.131238	-0.000817	0.744001
-0.378297	-0.415826	4.141235	-0.000798	0.744228
-0.214613	-0.338712	4.151232	-0.000832	0.744435
-0.275723	-0.207111	4.161229	-0.000823	0.744670
-0.120696	-0.096297	4.171226	-0.000855	0.744938
-0.033710	0.032254	4.181222	-0.000874	0.745217
0.000000	0.167785	4.191219	-0.000883	0.745491

0.212795	0.778825	4.196224	-0.000924	0.746726
0.533853	2.039824	4.201229	-0.000986	0.749224
0.860418	3.907463	4.206234	-0.001050	0.752859
1.257983	6.326488	4.211238	-0.001127	0.757531
1.610744	9.263201	4.216243	-0.001196	0.763121
2.239789	12.650225	4.221248	-0.001317	0.769591
2.580539	16.548690	4.226253	-0.001384	0.776845
2.813152	20.867274	4.231258	-0.001432	0.784757
3.406993	25.543540	4.236262	-0.001547	0.793343
3.688399	30.614605	4.241267	-0.001604	0.802436
4.061779	36.025017	4.246272	-0.001678	0.812047
4.570324	41.723474	4.251277	-0.001778	0.822084
5.076356	47.739165	4.256282	-0.001877	0.832538
5.745623	53.983429	4.261286	-0.002007	0.843295
6.194171	60.517116	4.266291	-0.002097	0.854331
6.514803	67.302275	4.271296	-0.002162	0.865601
7.062739	74.274165	4.276301	-0.002270	0.877093
7.400884	81.465680	4.281306	-0.002339	0.888726
8.588275	88.703705	4.286310	-0.002566	0.900517
10.616519	95.992708	4.291315	-0.002950	0.912462
11.181960	103.678342	4.296320	-0.003062	0.924467
11.919474	111.482941	4.301325	-0.003206	0.936544
15.016513	119.002035	4.306330	-0.003789	0.948655
15.668519	127.099656	4.311334	-0.003917	0.960836
16.296097	135.276986	4.316339	-0.004040	0.972973
17.201497	143.500791	4.321344	-0.004216	0.985097
17.504748	151.928485	4.326349	-0.004279	0.997214
18.363204	160.254221	4.331354	-0.004446	1.009177
19.803037	168.560139	4.336358	-0.004720	1.021112
20.736411	177.010140	4.341363	-0.004901	1.032986
21.286830	185.555864	4.346368	-0.005011	1.044764
22.150285	194.088902	4.351373	-0.005178	1.056466
22.783739	202.683213	4.356378	-0.005303	1.068067
23.349527	211.313904	4.361382	-0.005416	1.079576
24.038256	219.909566	4.366387	-0.005551	1.090946
25.525754	228.394197	4.371392	-0.005835	1.102231
26.084067	237.072219	4.376397	-0.005946	1.113444
26.707758	245.701606	4.381402	-0.006069	1.124498
27.468432	254.344400	4.386406	-0.006218	1.135490
28.182184	262.976372	4.391411	-0.006358	1.146353
28.896909	271.642796	4.396416	-0.006498	1.157156
30.261097	280.138882	4.401421	-0.006759	1.167787
30.695626	288.793470	4.406426	-0.006847	1.178321
31.248195	297.424668	4.411430	-0.006956	1.188757
31.854199	306.021286	4.416435	-0.007076	1.199072
32.616584	314.586951	4.421440	-0.007225	1.209294
33.779620	323.081776	4.426445	-0.007449	1.219426
34.433155	331.665025	4.431450	-0.007577	1.229477
35.003528	340.250696	4.436454	-0.007691	1.239433
35.649435	348.784471	4.441459	-0.007818	1.249264
36.379217	357.301564	4.446464	-0.007961	1.259016
37.220956	365.783255	4.451469	-0.008124	1.268674
37.661888	374.324368	4.456474	-0.008213	1.278249
38.384036	382.801267	4.461478	-0.008355	1.287735
38.802985	391.322544	4.466483	-0.008440	1.297144
39.444861	399.780663	4.471488	-0.008566	1.306457
40.184710	408.345984	4.476493	-0.008711	1.315836
40.795577	416.754646	4.481498	-0.008831	1.324959
41.534614	425.164532	4.486502	-0.008976	1.334042
42.273492	433.545072	4.491507	-0.009120	1.343034
42.726073	441.980629	4.496512	-0.009211	1.351972
43.500596	450.338001	4.501517	-0.009363	1.360826
44.103449	458.714098	4.506522	-0.009482	1.369613
44.654515	467.108462	4.511526	-0.009591	1.378353
45.420447	475.442893	4.516531	-0.009741	1.387013
46.095504	483.820471	4.521536	-0.009873	1.395647
46.144583	492.248700	4.526541	-0.009889	1.404175
46.694436	500.585550	4.531546	-0.009998	1.412642
47.439969	508.891299	4.536550	-0.010144	1.421060
48.276976	517.173697	4.541555	-0.010307	1.429420
48.744832	525.530020	4.546560	-0.010401	1.437744
49.257518	533.843746	4.551565	-0.010503	1.445985
49.876316	542.153288	4.556570	-0.010625	1.454193
50.508133	550.452100	4.561574	-0.010749	1.462345
50.950896	558.786484	4.566579	-0.010839	1.470457
51.434708	567.114357	4.571584	-0.010935	1.478524
52.050797	575.370693	4.576589	-0.011057	1.486500
52.463547	583.672321	4.581594	-0.011141	1.494444
53.097886	591.931376	4.586598	-0.011265	1.502340
53.568628	600.217433	4.591603	-0.011360	1.510195
53.933513	608.511599	4.596608	-0.011435	1.518000
54.411886	616.761860	4.601613	-0.011530	1.525742
55.015386	625.010872	4.606618	-0.011650	1.533462
55.676330	633.240074	4.611622	-0.011779	1.541134
55.807084	641.540763	4.616627	-0.011811	1.548754
56.333743	649.790048	4.621632	-0.011915	1.556348
56.895357	657.992708	4.626637	-0.012027	1.563868
57.469472	666.201841	4.631642	-0.012140	1.571360
57.907719	674.449261	4.636646	-0.012229	1.578830
58.380217	682.648713	4.641651	-0.012323	1.586227
58.773746	690.913994	4.646656	-0.012403	1.593637
58.958498	699.165189	4.651661	-0.012445	1.600971
59.688837	707.324632	4.656666	-0.012587	1.608267
60.279063	715.537497	4.661670	-0.012704	1.615557
60.676464	723.751849	4.666675	-0.012785	1.622788
61.239113	731.969592	4.671680	-0.012896	1.630014
61.879936	740.195217	4.676685	-0.013022	1.637224
62.140198	748.388349	4.681690	-0.013078	1.644323
62.693553	756.574258	4.686694	-0.013187	1.651425
63.047956	764.779343	4.691699	-0.013260	1.658485
63.491537	772.947225	4.696704	-0.013349	1.665496
63.856399	781.180624	4.701709	-0.013424	1.672522
64.007058	789.385477	4.706714	-0.013459	1.679466
64.537542	797.545297	4.711718	-0.013564	1.686394
64.909801	805.742206	4.716723	-0.013640	1.693304
65.399615	813.893512	4.721728	-0.013738	1.700163
65.941561	822.064435	4.726733	-0.013846	1.707017
66.543618	830.239308	4.731738	-0.013965	1.713855
66.772776	838.438062	4.736742	-0.014014	1.720637
67.263669	846.584155	4.741747	-0.014112	1.727382
67.800369	854.745508	4.746752	-0.014219	1.734120
68.095329	862.938961	4.751757	-0.014280	1.740826
68.403792	871.099739	4.756762	-0.014345	1.747482
69.132661	879.229870	4.761766	-0.014487	1.754141
69.548678	887.365194	4.766771	-0.014571	1.760739
69.587139	895.582256	4.771776	-0.014585	1.767331
70.200812	903.728133	4.776781	-0.014706	1.773913
70.384681	911.898314	4.781786	-0.014747	1.780437
70.656286	920.080544	4.786790	-0.014804	1.786957
71.114373	928.265672	4.791795	-0.014896	1.793478
71.508476	936.400751	4.796800	-0.014976	1.799929
71.928946	944.528651	4.801805	-0.015061	1.806354
72.433384	952.644758	4.806810	-0.015162	1.812757
73.050242	960.771354	4.811814	-0.015284	1.819159
73.547939	968.874784	4.816819	-0.015383	1.825506
73.978004	977.042191	4.821824	-0.015470	1.831872
74.569510	985.162533	4.826829	-0.015586	1.838199
74.684278	993.329916	4.831834	-0.015615	1.844484
75.163750	1001.468054	4.836838	-0.015711	1.850768
75.640499	1009.594761	4.841843	-0.015806	1.857021
76.158453	1017.711361	4.846848	-0.015909	1.863251
76.503028	1025.880207	4.851853	-0.015980	1.869479
76.871718	1034.022850	4.856858	-0.016055	1.875669
77.160583	1042.161468	4.861862	-0.016116	1.881827
77.769661	1050.254022	4.866867	-0.016236	1.887966
78.083160	1058.420413	4.871872	-0.016301	1.894107
78.694678	1066.504276	4.876877	-0.016422	1.900200
78.996206	1074.629130	4.881882	-0.016484	1.906270
79.321858	1082.796172	4.886886	-0.016552	1.912353
79.839797	1090.898463	4.891891	-0.016655	1.918391
80.313735	1098.993652	4.896896	-0.016750	1.924400
80.637945	1107.138821	4.901901	-0.016817	1.930410
80.710661	1115.299786	4.906906	-0.016837	1.936385
81.125819	1123.410858	4.911910	-0.016921	1.942343
81.424406	1131.533708	4.916915	-0.016983	1.948278
81.844552	1139.705725	4.921920	-0.017068	1.954244
82.398124	1147.750894	4.926925	-0.017178	1.960115
82.639172	1155.853431	4.931930	-0.017230	1.965976
83.181188	1163.963175	4.936934	-0.017337	1.971856
83.436009	1172.086415	4.941939	-0.017391	1.977698
84.107674	1180.137992	4.946944	-0.017523	1.983516
84.281454	1188.294086	4.951949	-0.017562	1.989338
84.559386	1196.416277	4.956954	-0.017620	1.995130
85.093062	1204.494850	4.961958	-0.017726	2.000901
85.594737	1212.569588	4.966963	-0.017827	2.006650
86.028342	1220.694865	4.971968	-0.017914	2.012410
86.384763	1228.809715	4.976973	-0.017987	2.018138
86.610144	1236.916271	4.981978	-0.018036	2.023831
87.130606	1245.019950	4.986982	-0.018139	2.029536
87.562093	1253.136794	4.991987	-0.018226	2.035225
87.645436	1261.262863	4.996992	-0.018248	2.040869
87.947664	1269.355949	5.001997	-0.018311	2.046497
88.213263	1277.454043	5.007002	-0.018368	2.052109
88.707543	1285.552958	5.012006	-0.018466	2.057729
89.304953	1293.607197	5.017011	-0.018584	2.063313
89.664024	1301.702478	5.022016	-0.018658	2.068886
90.204020	1309.816722	5.027021	-0.018765	2.074476
90.447825	1317.913613	5.032026	-0.018817	2.080009
90.644508	1326.023220	5.037030	-0.018860	2.085531
90.975207	1334.129308	5.042035	-0.018928	2.091049
91.539225	1342.199015	5.047040	-0.019040	2.096551
91.796221	1350.322435	5.052045	-0.019095	2.102045
92.055045	1358.402342	5.057050	-0.019150	2.107495
92.517323	1366.561609	5.062054	-0.019242	2.113004
92.828996	1374.643458	5.067059	-0.019307	2.118432
93.081054	1382.717792	5.072064	-0.019361	2.123835
93.563509	1390.774669	5.077069	-0.019457	2.129236
94.118439	1398.836345	5.082074	-0.019567	2.134632
94.406995	1406.932158	5.087078	-0.019627	2.140012
94.653171	1415.014109	5.092083	-0.019680	2.145365
94.649747	1423.162290	5.097088	-0.019686	2.150725
95.272719	1431.214877	5.102093	-0.019809	2.156068
95.619601	1439.278261	5.107098	-0.019880	2.161378
96.123768	1447.340842	5.112102	-0.019980	2.166690
96.526860	1455.433869	5.117107	-0.020062	2.171999
96.961576	1463.511264	5.122112	-0.020150	2.177287
97.167245	1471.628272	5.127117	-0.020195	2.182567
97.507922	1479.705422	5.132122	-0.020265	2.187821
97.663438	1487.858920	5.137126	-0.020300	2.193095
98.027171	1495.905681	5.142131	-0.020375	2.198306
98.414939	1503.964545	5.147136	-0.020454	2.203515
98.978924	1512.013870	5.152141	-0.020565	2.208721
98.941372	1520.155772	5.157146	-0.020565	2.213920
99.328111	1528.227929	5.162150	-0.020644	2.219100
99.601474	1536.281780	5.167155	-0.020701	2.224247
100.048531	1544.358806	5.172160	-0.020791	2.229411
100.433567	1552.456889	5.177165	-0.020869	2.234571
100.771333	1560.509052	5.182170	-0.020939	2.239686
101.020444	1568.583288	5.187174	-0.020992	2.244796
101.390002	1576.650184	5.192179	-0.021067	2.249899
102.032078	1584.727525	5.197184	-0.021194	2.255022
102.524412	1592.809988	5.202189	-0.021292	2.260122
102.676484	1600.880801	5.207194	-0.021327	2.265175
103.103648	1608.989712	5.212198	-0.021413	2.270263
103.406634	1617.128483	5.217203	-0.021476	2.275348
103.626545	1625.180964	5.222208	-0.021524	2.280361
103.893711	1633.242815	5.227213	-0.021580	2.285373
104.533118	1641.259293	5.232218	-0.021706	2.290377
104.504637	1649.406928	5.237222	-0.021707	2.295395
104.738500	1657.451551	5.242227	-0.021758	2.300360
105.191791	1665.479906	5.247232	-0.021849	2.305323
105.634450	1673.559515	5.252237	-0.021938	2.310306
105.775385	1681.653512	5.257242	-0.021971	2.315262
106.230536	1689.685768	5.262246	-0.022062	2.320195
106.557226	1697.739811	5.267251	-0.022129	2.325120
107.027372	1705.795559	5.272256	-0.022224	2.330048
107.339589	1713.905336	5.277261	-0.022288	2.334985
107.911467	1721.918740	5.282266	-0.022401	2.339875
108.273628	1729.999428	5.287270	-0.022476	2.344777
108.372858	1738.115121	5.292275	-0.022501	2.349669
108.653613	1746.209034	5.297280	-0.022560	2.354553
109.204286	1754.248168	5.302285	-0.022669	2.359415
109.466292	1762.287141	5.307290	-0.022724	2.364244
109.756697	1770.375067	5.312294	-0.022785	2.369094
110.011113	1778.449441	5.317299	-0.022839	2.373924
110.208853	1786.530148	5.322304	-0.022882	2.378742
110.558771	1794.568333	5.327309	-0.022954	2.383538
110.826170	1802.634755	5.332314	-0.023011	2.388335
111.184408	1810.728500	5.337318	-0.023084	2.393145
111.272421	1818.804218	5.342323	-0.023107	2.397913
111.666574	1826.823826	5.347328	-0.023187	2.402663
112.379580	1834.852958	5.352333	-0.023327	2.407433
112.313638	1842.958708	5.357338	-0.023321	2.412179
112.706990	1851.038641	5.362342	-0.023401	2.416936
113.041928	1859.086531	5.367347	-0.023470	2.421660
113.363099	1867.137969	5.372352	-0.023536	2.426376
113.836734	1875.241128	5.377357	-0.023631	2.431124
114.146524	1883.329479	5.382362	-0.023695	2.435842
114.428829	1891.381221	5.387366	-0.023755	2.440527
114.659548	1899.418360	5.392371	-0.023804	2.445191
114.867003	1907.462949	5.397376	-0.023850	2.449849
115.157182	1915.548006	5.402381	-0.023910	2.454527
115.477120	1923.581195	5.407386	-0.023976	2.459168
115.793074	1931.637383	5.412390	-0.024042	2.463814
116.121520	1939.698637	5.417395	-0.024110	2.468455
116.341330	1947.772714	5.422400	-0.024157	2.473086
116.624905	1955.843133	5.427405	-0.024217	2.477711
116.836060	1963.871241	5.432410	-0.024263	2.482298
117.133119	1971.932663	5.437414	-0.024325	2.486902
117.240030	1980.024674	5.442419	-0.024351	2.491500
117.568636	1988.055138	5.447424	-0.024419	2.496072
117.767750	1996.128816	5.452429	-0.024463	2.500650
118.072857	2004.166702	5.457434	-0.024526	2.505207
118.389947	2012.231210	5.462438	-0.024592	2.509771
119.048830	2020.289642	5.467443	-0.024721	2.514349
119.877812	2028.274881	5.472448	-0.024882	2.518889
120.133552	2036.341543	5.477453	-0.024936	2.523425
120.310206	2044.398877	5.482458	-0.024976	2.527942
120.780810	2052.477298	5.487462	-0.025070	2.532484
120.872191	2060.559810	5.492467	-0.025094	2.536993
121.314056	2068.596852	5.497472	-0.025183	2.541493
121.759249	2076.633651	5.502477	-0.025272	2.545985
121.791164	2084.715206	5.507482	-0.025285	2.550466
122.068249	2092.795018	5.512486	-0.025343	2.554954
122.305434	2100.841053	5.517491	-0.025394	2.559413
122.756756	2108.848243	5.522496	-0.025485	2.563858
123.004488	2116.938655	5.527501	-0.025537	2.568327
123.276888	2124.987316	5.532506	-0.025595	2.572766
123.654448	2133.047145	5.537510	-0.025672	2.577212
124.109680	2141.071167	5.542515	-0.025763	2.581635
124.166746	2149.152393	5.547520	-0.025780	2.586055
124.457005	2157.237034	5.552525	-0.025841	2.590484
124.702710	2165.438811	5.557530	-0.025894	2.594967
124.996597	2173.444868	5.562534	-0.025955	2.599339
125.420743	2181.417047	5.567539	-0.026040	2.603694
125.933517	2189.408299	5.572544	-0.026143	2.608058
126.321371	2197.472334	5.577549	-0.026221	2.612446
126.535394	2205.523027	5.582554	-0.026268	2.616807
126.989381	2213.562051	5.587558	-0.026359	2.621171
127.278458	2221.591508	5.592563	-0.026419	2.625511
127.350378	2229.657931	5.597568	-0.026440	2.629850
127.943228	2237.720121	5.602573	-0.026557	2.634213
128.248435	2245.747837	5.607578	-0.026620	2.638531
128.461337	2253.800776	5.612582	-0.026666	2.642850
128.754130	2261.831217	5.617587	-0.026727	2.647156
128.706771	2269.915805	5.622592	-0.026725	2.651460
129.022380	2277.988423	5.627597	-0.026791	2.655775
129.187795	2286.004370	5.632602	-0.026828	2.660043
129.551678	2294.042221	5.637606	-0.026903	2.664329
129.957451	2302.084034	5.642611	-0.026985	2.668612
130.168481	2310.173807	5.647616	-0.027031	2.672902
130.601843	2318.222628	5.652621	-0.027118	2.677177
131.037082	2326.210215	5.657626	-0.027206	2.681413
131.137157	2334.275394	5.662630	-0.027231	2.685661
131.447070	2342.309758	5.667635	-0.027295	2.689900
131.885935	2350.358208	5.672640	-0.027384	2.694148
132.141579	2358.426053	5.677645	-0.027438	2.698388
132.128953	2366.486215	5.682650	-0.027442	2.702600
132.480854	2374.534007	5.687654	-0.027514	2.706822
132.808612	2382.571071	5.692659	-0.027582	2.711030
133.040812	2390.645408	5.697664	-0.027632	2.715245
133.303522	2398.663245	5.702669	-0.027687	2.719426
133.656900	2406.674398	5.707674	-0.027760	2.723603
134.220843	2414.698482	5.712678	-0.027871	2.727792
134.380459	2422.795717	5.717683	-0.027908	2.731989
134.578696	2430.865237	5.722688	-0.027951	2.736167
134.980497	2438.892930	5.727693	-0.028033	2.740329
135.196621	2446.916047	5.732698	-0.028080	2.744471
135.621158	2454.959791	5.737702	-0.028165	2.748630
135.868098	2463.085507	5.742707	-0.028218	2.752814
135.924596	2471.153314	5.747712	-0.028235	2.756951
136.249085	2479.173884	5.752717	-0.028302	2.761073
136.392364	2487.159251	5.757722	-0.028335	2.765161
136.798134	2495.198263	5.762726	-0.028418	2.769285
137.040228	2503.267909	5.767731	-0.028469	2.773409
137.324994	2511.286390	5.772736	-0.028529	2.777503
137.840146	2519.320347	5.777741	-0.028632	2.781612
137.963046	2527.361303	5.782746	-0.028661	2.785696
138.295639	2535.409071	5.787750	-0.028730	2.789790
138.506085	2543.478606	5.792755	-0.028775	2.793881
138.817089	2551.500869	5.797760	-0.028840	2.797948
139.136141	2559.547706	5.802765	-0.028906	2.802023
139.365121	2567.568967	5.807770	-0.028955	2.806073
139.725860	2575.610505	5.812774	-0.029029	2.810135
140.191181	2583.656305	5.817779	-0.029122	2.814199
140.384935	2591.708188	5.822784	-0.029165	2.818245
140.571373	2599.776965	5.827789	-0.029206	2.822293
140.738310	2607.814634	5.832794	-0.029244	2.826318
141.111044	2615.857429	5.837798	-0.029320	2.830352
141.389420	2623.912570	5.842803	-0.029379	2.834381
141.684487	2631.914648	5.847808	-0.029440	2.838379
141.860773	2639.972405	5.852813	-0.029480	2.842392
142.013584	2648.011553	5.857818	-0.029515	2.846389
142.349633	2656.037705	5.862822	-0.029584	2.850384
142.665628	2664.089566	5.867827	-0.029649	2.854385
143.001830	2672.105740	5.872832	-0.029719	2.858363
143.334629	2680.146962	5.877837	-0.029787	2.862348
143.535570	2688.185134	5.882842	-0.029831	2.866319
143.883207	2696.249979	5.887846	-0.029903	2.870306
144.300912	2704.296182	5.892851	-0.029987	2.874281
144.418992	2712.344376	5.897856	-0.030016	2.878236
144.768592	2720.368476	5.902861	-0.030087	2.882186
145.061042	2728.384566	5.907866	-0.030149	2.886123
145.487260	2736.438564	5.912870	-0.030235	2.890081
145.931257	2744.483955	5.917875	-0.030324	2.894030
145.935238	2752.548630	5.922880	-0.030331	2.897960
146.211991	2760.588508	5.927885	-0.030389	2.901886
146.282094	2768.616451	5.932890	-0.030409	2.905791
146.674379	2776.668254	5.937894	-0.030489	2.909718
146.984179	2784.780155	5.942899	-0.030553	2.913665
147.098115	2792.792245	5.947904	-0.030581	2.917549
147.402878	2800.808523	5.952909	-0.030644	2.921439
147.653637	2808.793625	5.957914	-0.030698	2.925306
147.977969	2816.817757	5.962918	-0.030765	2.929190
148.221462	2824.899132	5.967923	-0.030817	2.933092
148.524679	2832.923206	5.972928	-0.030880	2.936965
148.838601	2840.964701	5.977933	-0.030945	2.940842
148.883981	2848.971623	5.982938	-0.030960	2.944683
149.327823	2857.027756	5.987942	-0.031049	2.948563
149.638895	2865.097893	5.992947	-0.031114	2.952438
149.989880	2873.126771	5.997952	-0.031186	2.956290
150.069219	2881.161958	6.002957	-0.031207	2.960126
150.319724	2889.170982	6.007962	-0.031260	2.963953
151.006409	2897.186724	6.012966	-0.031395	2.967800
151.189384	2905.253003	6.017971	-0.031435	2.971641
151.233228	2913.316937	6.022976	-0.031450	2.975469
151.497802	2921.356034	6.027981	-0.031506	2.979292
151.635980	2929.369454	6.032986	-0.031539	2.983090
151.812525	2937.424161	6.037990	-0.031578	2.986906
152.085170	2945.462598	6.042995	-0.031635	2.990713
152.254936	2953.522917	6.048000	-0.031674	2.994521
152.651947	2961.553152	6.053005	-0.031754	2.998321
153.059591	2969.516929	6.058010	-0.031837	3.002086
153.333551	2977.561460	6.063014	-0.031894	3.005877
153.712546	2985.559373	6.068019	-0.031972	3.009646
154.164842	2993.595239	6.073024	-0.032062	3.013433
154.353236	3001.677584	6.078029	-0.032104	3.017223
154.492472	3009.703084	6.083034	-0.032137	3.020979
154.739370	3017.724826	6.088038	-0.032189	3.024734
155.084546	3025.789420	6.093043	-0.032260	3.028509
155.352448	3033.827943	6.098048	-0.032317	3.032264
155.590721	3041.903826	6.103053	-0.032368	3.036030
155.799773	3049.892616	6.108058	-0.032413	3.039749
156.210062	3057.894241	6.113062	-0.032496	3.043479
156.427823	3065.947209	6.118067	-0.032543	3.047219
156.723802	3073.973160	6.123072	-0.032605	3.050946
157.068877	3082.051415	6.128077	-0.032676	3.054694
157.308155	3090.072020	6.133082	-0.032727	3.058407
157.726683	3098.092423	6.138086	-0.032812	3.062123
157.857745	3106.147881	6.143091	-0.032843	3.065837
158.047402	3114.176676	6.148096	-0.032885	3.069537
158.375557	3122.306050	6.153101	-0.032953	3.073286
158.657388	3130.294893	6.158106	-0.033012	3.076963
159.053321	3138.288785	6.163110	-0.033092	3.080643
159.256468	3146.310447	6.168115	-0.033136	3.084323
159.346167	3154.349758	6.173120	-0.033160	3.088001
159.599485	3162.423409	6.178125	-0.033214	3.091697
159.701644	3170.458227	6.183130	-0.033239	3.095365
159.877534	3178.475395	6.188134	-0.033279	3.099024
160.089463	3186.473138	6.193139	-0.033325	3.102671
160.470581	3194.493189	6.198144	-0.033402	3.106331
160.878139	3202.534057	6.203149	-0.033485	3.109998
160.718061	3210.626276	6.208154	-0.033462	3.113658
161.123088	3218.634232	6.213158	-0.033544	3.117302
161.737200	3226.636022	6.218163	-0.033665	3.120947
161.783611	3234.632718	6.223168	-0.033680	3.124560
162.172034	3242.706279	6.228173	-0.033759	3.128219
162.432283	3250.745882	6.233178	-0.033814	3.131853
162.706390	3258.785976	6.238182	-0.033872	3.135483
162.987799	3266.797989	6.243187	-0.033931	3.139097
163.214624	3274.813566	6.248192	-0.033979	3.142706
163.481272	3282.881289	6.253197	-0.034036	3.146335
163.560858	3290.920804	6.258202	-0.034057	3.149940
164.014930	3298.950824	6.263206	-0.034148	3.153552
164.494401	3306.984347	6.268211	-0.034244	3.157163
164.612430	3315.006138	6.273216	-0.034273	3.160749
164.964715	3323.015298	6.278221	-0.034345	3.164335
165.225066	3331.033429	6.283226	-0.034400	3.167918
165.423466	3339.108842	6.288230	-0.034444	3.171519
165.561962	3347.166222	6.293235	-0.034476	3.175105
165.923510	3355.163671	6.298240	-0.034550	3.178670
166.434017	3363.185011	6.303245	-0.034652	3.182248
166.449244	3371.213982	6.308250	-0.034661	3.185804
166.891110	3379.243311	6.313254	-0.034750	3.189374
167.038676	3387.313930	6.318259	-0.034784	3.192946
167.304786	3395.340729	6.323264	-0.034840	3.196500
167.502001	3403.373168	6.328269	-0.034884	3.200050
167.801120	3411.355404	6.333274	-0.034946	3.203577
168.094317	3419.412490	6.338278	-0.035007	3.207133
168.566966	3427.441983	6.343283	-0.035102	3.210681
168.732177	3435.493641	6.348288	-0.035139	3.214222
169.177212	3443.508254	6.353293	-0.035229	3.217754
169.241961	3451.550131	6.358298	-0.035247	3.221278
169.473230	3459.546135	6.363302	-0.035297	3.224785
169.935863	3467.585320	6.368307	-0.035390	3.228317
170.045243	3475.660447	6.373312	-0.035417	3.231846
170.333072	3483.739485	6.378317	-0.035477	3.235380
170.711417	3491.705856	6.383322	-0.035554	3.238865
170.864441	3499.721785	6.388326	-0.035589	3.242358
171.279955	3507.742537	6.393331	-0.035673	3.245861
171.641763	3515.718066	6.398336	-0.035747	3.249337
171.830399	3523.813927	6.403341	-0.035789	3.252855
172.025163	3531.827952	6.408346	-0.035832	3.256335
172.371495	3539.839060	6.413350	-0.035903	3.259815
172.671982	3547.871735	6.418355	-0.035966	3.263299
172.622867	3555.923048	6.423360	-0.035963	3.266773
172.881835	3563.976860	6.428365	-0.036018	3.270257
173.012123	3572.036478	6.433370	-0.036049	3.273734
173.365088	3580.031035	6.438374	-0.036121	3.277189
173.760563	3588.020954	6.443379	-0.036201	3.280639
173.953305	3596.028886	6.448384	-0.036244	3.284086
174.133629	3604.119255	6.453389	-0.036284	3.287564
174.351990	3612.135455	6.458394	-0.036331	3.291008
174.552570	3620.194583	6.463398	-0.036375	3.294466
174.994588	3628.202909	6.468403	-0.036464	3.297908
174.996957	3636.230182	6.473408	-0.036471	3.301337
175.434231	3644.239157	6.478413	-0.036559	3.304772
175.572163	3652.277907	6.483418	-0.036592	3.308204
175.835834	3660.335312	6.488422	-0.036647	3.311645
176.053737	3668.392765	6.493427	-0.036695	3.315081
176.073877	3676.387781	6.498432	-0.036705	3.318480
176.605815	3684.401549	6.503437	-0.036811	3.321902
176.692313	3692.389702	6.508442	-0.036833	3.325293
177.168625	3700.397920	6.513446	-0.036929	3.328704
177.262349	3708.477266	6.518451	-0.036953	3.332127
177.429640	3716.511330	6.523456	-0.036991	3.335530
177.485684	3724.547755	6.528461	-0.037008	3.338926
177.759944	3732.544006	6.533466	-0.037065	3.342310
178.198166	3740.566293	6.538470	-0.037154	3.345707
178.468092	3748.610631	6.543475	-0.037210	3.349104
178.648261	3756.655354	6.548480	-0.037251	3.352495
178.963191	3764.716154	6.553485	-0.037316	3.355893
179.215001	3772.719221	6.558490	-0.037369	3.359262
179.307119	3780.748476	6.563494	-0.037393	3.362633
179.626518	3788.752428	6.568499	-0.037459	3.365997
180.059923	3796.743725	6.573504	-0.037547	3.369357
180.373859	3804.826505	6.578509	-0.037612	3.372748
180.450111	3812.890449	6.583514	-0.037633	3.376118
180.807092	3820.860341	6.588518	-0.037706	3.379456
181.066312	3828.901930	6.593523	-0.037760	3.382818
181.372413	3836.902729	6.598528	-0.037824	3.386160
181.507848	3844.973862	6.603533	-0.037856	3.389522
181.859370	3853.044148	6.608538	-0.037928	3.392889
182.048758	3861.096944	6.613542	-0.037970	3.396238
182.142312	3869.067811	6.618547	-0.037994	3.399548
182.288581	3877.037626	6.623552	-0.038028	3.402855
182.685355	3885.090489	6.628557	-0.038108	3.406202
182.903795	3893.076985	6.633562	-0.038156	3.409513
183.302243	3901.138269	6.638566	-0.038236	3.412857
183.473728	3909.208799	6.643571	-0.038275	3.416193
183.563728	3917.169712	6.648576	-0.038298	3.419479
183.890038	3925.212388	6.653581	-0.038366	3.422803
184.121762	3933.220623	6.658586	-0.038415	3.426106
184.412905	3941.258490	6.663590	-0.038476	3.429421
184.840916	3949.301597	6.668595	-0.038563	3.432738
185.072919	3957.334989	6.673600	-0.038612	3.436042
185.322579	3965.353478	6.678605	-0.038666	3.439338
185.757846	3973.351943	6.683610	-0.038753	3.442628
185.936555	3981.387184	6.688614	-0.038793	3.445921
186.210641	3989.463104	6.693619	-0.038851	3.449231
186.239764	3997.481500	6.698624	-0.038863	3.452506
186.714596	4005.545669	6.703629	-0.038958	3.455812
186.742406	4013.527486	6.708634	-0.038970	3.459066
187.009792	4021.571570	6.713638	-0.039026	3.462350
187.331223	4029.586152	6.718643	-0.039093	3.465620
187.604503	4037.585348	6.723648	-0.039150	3.468880
187.843952	4045.647172	6.728653	-0.039201	3.472161
188.151653	4053.699858	6.733658	-0.039265	3.475437
188.437059	4061.684956	6.738662	-0.039325	3.478682
188.836289	4069.695031	6.743667	-0.039406	3.481938
188.942517	4077.689969	6.748672	-0.039432	3.485175
189.095217	4085.746004	6.753677	-0.039467	3.488435
189.223941	4093.765860	6.758682	-0.039498	3.491677
189.388357	4101.812950	6.763686	-0.039535	3.494928
189.644279	4109.816409	6.768691	-0.039589	3.498161
189.913534	4117.842673	6.773696	-0.039646	3.501401
189.989338	4125.862553	6.778701	-0.039667	3.504629
190.127035	4133.885934	6.783706	-0.039699	3.507858
190.368171	4141.944707	6.788710	-0.039751	3.511100
190.744282	4149.980573	6.793715	-0.039827	3.514335
190.928640	4157.973831	6.798720	-0.039868	3.517544
191.388637	4165.995044	6.803725	-0.039961	3.520769
191.498955	4173.989230	6.808730	-0.039988	3.523970
191.519063	4182.060825	6.813734	-0.039998	3.527196
191.870175	4190.090809	6.818739	-0.040070	3.530413
192.135416	4198.133914	6.823744	-0.040126	3.533629
192.522209	4206.194244	6.828749	-0.040205	3.536853
192.705894	4214.162659	6.833754	-0.040246	3.540031
192.790159	4222.182595	6.838758	-0.040268	3.543224
192.900328	4230.271561	6.843763	-0.040295	3.546442
193.015731	4238.242476	6.848768	-0.040323	3.549611
193.633859	4246.331670	6.853773	-0.040445	3.552838
193.830865	4254.393956	6.858778	-0.040488	3.556039
193.827663	4262.366227	6.863782	-0.040494	3.559196
194.271362	4270.365919	6.868787	-0.040583	3.562374
194.512619	4278.345007	6.873792	-0.040635	3.565535
194.647458	4286.376972	6.878797	-0.040667	3.568711
194.607195	4294.428819	6.883802	-0.040666	3.571887
195.128127	4302.428361	6.888806	-0.040769	3.575056
195.561601	4310.452638	6.893811	-0.040857	3.578229
195.486495	4318.481808	6.898816	-0.040849	3.581386
195.882101	4326.449436	6.903821	-0.040930	3.584530
196.262732	4334.511193	6.908826	-0.041007	3.587708
196.472528	4342.549451	6.913830	-0.041053	3.590868
196.576097	4350.608004	6.918835	-0.041079	3.594031
196.511475	4358.598702	6.923840	-0.041073	3.597160
196.911339	4366.592318	6.928845	-0.041154	3.600300
197.231541	4374.598706	6.933850	-0.041221	3.603440
197.439926	4382.658442	6.938854	-0.041266	3.606596
197.603026	4390.684504	6.943859	-0.041303	3.609734
197.801116	4398.706386	6.948864	-0.041347	3.612868
198.110412	4406.774892	6.953869	-0.041411	3.616021
198.326891	4414.759962	6.958874	-0.041458	3.619136
198.673373	4422.810475	6.963878	-0.041529	3.622277
198.893976	4430.807714	6.968883	-0.041577	3.625392
199.099395	4438.838719	6.973888	-0.041621	3.628516
199.535184	4446.882698	6.978893	-0.041709	3.631649
199.646885	4454.938252	6.983898	-0.041737	3.634775
200.005598	4462.952524	6.988902	-0.041810	3.637889
200.202290	4470.969508	6.993907	-0.041853	3.640997
200.278774	4478.929694	6.998912	-0.041874	3.644077
200.471354	4486.991490	7.003917	-0.041917	3.647197
200.564901	4494.986852	7.008922	-0.041941	3.650286
200.862802	4503.047390	7.013926	-0.042003	3.653403
201.145588	4511.085168	7.018931	-0.042062	3.656508
201.100346	4519.085296	7.023936	-0.042060	3.659587
201.300295	4527.144843	7.028941	-0.042104	3.662693
201.690865	4535.121483	7.033946	-0.042183	3.665769
201.779072	4543.138029	7.038950	-0.042206	3.668850
202.165797	4551.195392	7.043955	-0.042285	3.671952
202.363448	4559.200499	7.048960	-0.042328	3.675026
202.757906	4567.219069	7.053965	-0.042409	3.678108
203.181640	4575.211629	7.058970	-0.042494	3.681177
203.379276	4583.213547	7.063974	-0.042537	3.684243
203.714046	4591.286884	7.068979	-0.042606	3.687336
203.639625	4599.307771	7.073984	-0.042599	3.690396
204.073570	4607.324564	7.078989	-0.042687	3.693465
204.064453	4615.370205	7.083994	-0.042692	3.696532
204.344473	4623.352301	7.088998	-0.042750	3.699578
204.791724	4631.414955	7.094003	-0.042840	3.702657
205.022395	4639.402232	7.099008	-0.042890	3.705700
205.141417	4647.446864	7.104013	-0.042919	3.708759
205.422175	4655.495352	7.109018	-0.042977	3.711820
205.785502	4663.583287	7.114022	-0.043052	3.714897
206.006040	4671.584063	7.119027	-0.043099	3.717934
206.079769	4679.545442	7.124032	-0.043120	3.720950
206.375305	4687.540712	7.129037	-0.043181	3.723982
206.377600	4695.574167	7.134042	-0.043188	3.727018
206.735060	4703.572236	7.139046	-0.043262	3.730048
207.002345	4711.607399	7.144051	-0.043318	3.733086
207.519801	4719.634598	7.149056	-0.043421	3.736125
207.792394	4727.643044	7.154061	-0.043478	3.739149
207.726044	4735.678099	7.159066	-0.043473	3.742172
208.015757	4743.690353	7.164070	-0.043533	3.745193
208.290916	4751.744175	7.169075	-0.043591	3.748226
208.452993	4759.778266	7.174080	-0.043628	3.751247
208.561489	4767.836317	7.179085	-0.043655	3.754273
208.907206	4775.843266	7.184090	-0.043726	3.757283
209.138105	4783.817863	7.189094	-0.043775	3.760276
209.476996	4791.851681	7.194099	-0.043845	3.763291
209.449913	4799.880609	7.199104	-0.043847	3.766293
209.749568	4807.911489	7.204109	-0.043909	3.769301
209.881426	4815.994036	7.209114	-0.043940	3.772322
210.201372	4823.969020	7.214118	-0.044006	3.775305
210.544449	4831.989307	7.219123	-0.044077	3.778303
210.479303	4840.002434	7.224128	-0.044071	3.781287
210.763768	4847.994641	7.229133	-0.044131	3.784268
211.020497	4856.044454	7.234138	-0.044185	3.787267
211.188860	4864.063902	7.239142	-0.044223	3.790251
211.509497	4872.140627	7.244147	-0.044290	3.793258
211.956615	4880.121467	7.249152	-0.044380	3.796229
212.089090	4888.117653	7.254157	-0.044411	3.799196
212.041200	4896.140649	7.259162	-0.044408	3.802167
212.485973	4904.102862	7.264166	-0.044498	3.805124
212.603324	4912.153506	7.269171	-0.044526	3.808104
212.590394	4920.180749	7.274176	-0.044531	3.811071
212.922120	4928.247986	7.279181	-0.044599	3.814057
213.134248	4936.278522	7.284186	-0.044645	3.817025
213.261740	4944.231235	7.289190	-0.044675	3.819960
213.531456	4952.290657	7.294195	-0.044732	3.822935
213.768897	4960.259877	7.299200	-0.044783	3.825874
213.946715	4968.309981	7.304205	-0.044823	3.828838
214.072539	4976.365053	7.309210	-0.044853	3.831802
214.110350	4984.386226	7.314214	-0.044867	3.834749
214.611193	4992.444232	7.319219	-0.044966	3.837716
214.621430	5000.394278	7.324224	-0.044975	3.840632
214.896957	5008.417681	7.329229	-0.045033	3.843577
215.118487	5016.441785	7.334234	-0.045081	3.846520
215.175084	5024.470007	7.339238	-0.045098	3.849458
215.261627	5032.535242	7.344243	-0.045121	3.852409
215.457863	5040.525549	7.349248	-0.045164	3.855331
216.022242	5048.589497	7.354253	-0.045276	3.858286
215.880507	5056.590671	7.359258	-0.045256	3.861202
216.232916	5064.586893	7.364262	-0.045328	3.864123
216.484286	5072.641012	7.369267	-0.045381	3.867061
216.663766	5080.635666	7.374272	-0.045421	3.869974
216.993397	5088.814893	7.379277	-0.045490	3.872955
217.237775	5096.882997	7.384282	-0.045542	3.875891
217.568541	5104.797967	7.389286	-0.045610	3.878771
217.704019	5112.811809	7.394291	-0.045642	3.881681
218.102870	5120.690532	7.399296	-0.045722	3.884545
218.197771	5128.778087	7.404301	-0.045747	3.887476
218.379400	5136.772412	7.409306	-0.045787	3.890373
218.658483	5144.790225	7.414310	-0.045846	3.893279
218.810204	5152.886356	7.419315	-0.045881	3.896208
218.893229	5160.819202	7.424320	-0.045903	3.899074
219.101094	5168.892652	7.429325	-0.045948	3.901992
219.462264	5176.825913	7.434330	-0.046022	3.904860
219.792784	5184.901058	7.439334	-0.046090	3.907776
219.717750	5192.947244	7.444339	-0.046083	3.910671
220.000841	5200.950208	7.449344	-0.046142	3.913556
220.507191	5208.991518	7.454349	-0.046243	3.916457
220.650346	5216.952725	7.459354	-0.046276	3.919319
220.796420	5225.000587	7.464358	-0.046310	3.922211
220.980457	5232.988168	7.469363	-0.046351	3.925080
221.019409	5241.020162	7.474368	-0.046365	3.927960
221.223730	5249.050872	7.479373	-0.046409	3.930841
221.329198	5257.128154	7.484378	-0.046436	3.933734
221.512683	5265.123834	7.489382	-0.046477	3.936597
221.786214	5273.103601	7.494387	-0.046534	3.939454
221.923801	5281.106316	7.499392	-0.046566	3.942315
222.334802	5289.128954	7.504397	-0.046649	3.945185
222.080598	5297.219981	7.509402	-0.046609	3.948066
222.410681	5305.195311	7.514406	-0.046677	3.950914
223.016958	5313.272241	7.519411	-0.046796	3.953801
223.478047	5321.273536	7.524416	-0.046889	3.956656
223.713916	5329.205300	7.529421	-0.046939	3.959480
223.958001	5337.267265	7.534426	-0.046991	3.962349
224.173185	5345.225704	7.539430	-0.047038	3.965179
224.362523	5353.300272	7.544435	-0.047080	3.968047
224.624207	5361.289353	7.549440	-0.047135	3.970884
225.103021	5369.368626	7.554445	-0.047231	3.973754
225.210257	5377.419771	7.559450	-0.047258	3.976606
225.477989	5385.372345	7.564454	-0.047314	3.979424
225.655311	5393.422233	7.569459	-0.047354	3.982273
225.625173	5401.418372	7.574464	-0.047355	3.985098
225.736913	5409.492548	7.579469	-0.047382	3.987950
225.943961	5417.485081	7.584474	-0.047427	3.990773
226.313036	5425.502737	7.589478	-0.047503	3.993605
226.552457	5433.594946	7.594483	-0.047554	3.996459
226.743493	5441.551459	7.599488	-0.047596	3.999263
227.152967	5449.568864	7.604493	-0.047679	4.002090
227.258987	5457.570740	7.609498	-0.047705	4.004904
227.209960	5465.611723	7.614502	-0.047703	4.007728
227.508426	5473.653096	7.619507	-0.047765	4.010556
227.753295	5481.663416	7.624512	-0.047817	4.013369
227.962728	5489.722871	7.629517	-0.047863	4.016197
228.128304	5497.707949	7.634522	-0.047900	4.018997
228.414339	5505.738164	7.639526	-0.047960	4.021812
228.699338	5513.734894	7.644531	-0.048020	4.024613
228.598313	5521.751811	7.649536	-0.048008	4.027414
229.074073	5529.767959	7.654541	-0.048103	4.030221
229.116459	5537.874219	7.659546	-0.048117	4.033051
229.485139	5545.877727	7.664550	-0.048193	4.035848
229.647307	5553.863238	7.669555	-0.048229	4.038634
229.770489	5561.887330	7.674560	-0.048259	4.041431
229.953074	5569.855387	7.679565	-0.048300	4.044207
229.973472	5577.851782	7.684570	-0.048310	4.046988
230.147022	5585.856468	7.689574	-0.048349	4.049773
230.305861	5593.924887	7.694579	-0.048385	4.052578
230.600300	5601.934139	7.699584	-0.048447	4.055362
230.875420	5609.961507	7.704589	-0.048504	4.058151
231.021206	5617.964529	7.709594	-0.048538	4.060927
231.140707	5625.969632	7.714598	-0.048567	4.063701
231.328739	5634.020874	7.719603	-0.048609	4.066491
231.558047	5641.985828	7.724608	-0.048658	4.069249
231.625733	5650.071921	7.729613	-0.048677	4.072045
231.803149	5658.102393	7.734618	-0.048717	4.074821
232.119778	5666.096861	7.739622	-0.048782	4.077585
232.472793	5674.084634	7.744627	-0.048855	4.080345
232.673589	5682.081980	7.749632	-0.048899	4.083105
232.688737	5690.110928	7.754637	-0.048908	4.085871
232.905127	5698.144072	7.759642	-0.048955	4.088639
233.121822	5706.157331	7.764646	-0.049002	4.091399
233.554077	5714.208005	7.769651	-0.049089	4.094172
233.664482	5722.214495	7.774656	-0.049116	4.096924
233.743468	5730.208486	7.779661	-0.049138	4.099670
233.873411	5738.291571	7.784666	-0.049169	4.102445
234.107537	5746.242468	7.789670	-0.049219	4.105174
234.577114	5754.295923	7.794675	-0.049313	4.107939
234.528751	5762.304461	7.799680	-0.049310	4.110680
234.905144	5770.379695	7.804685	-0.049387	4.113448
235.266648	5778.397133	7.809690	-0.049461	4.116194
235.062712	5786.392719	7.814694	-0.049430	4.118923
235.360501	5794.410497	7.819699	-0.049492	4.121665
235.592335	5802.350042	7.824704	-0.049541	4.124377
235.643068	5810.444143	7.829709	-0.049558	4.127137
235.944460	5818.457971	7.834714	-0.049620	4.129872
236.145168	5826.488074	7.839718	-0.049664	4.132609
236.502590	5834.511769	7.844723	-0.049737	4.135344
236.415039	5842.548842	7.849728	-0.049728	4.138076
236.691800	5850.571433	7.854733	-0.049786	4.140806
236.839573	5858.560598	7.859738	-0.049820	4.143521
236.929708	5866.580019	7.864742	-0.049843	4.146244
237.187373	5874.609277	7.869747	-0.049898	4.148971
237.339436	5882.600462	7.874752	-0.049933	4.151681
237.755389	5890.652744	7.879757	-0.050017	4.154414
237.804406	5898.713360	7.884762	-0.050033	4.157143
238.224723	5906.626836	7.889766	-0.050118	4.159825
238.211752	5914.665924	7.894771	-0.050122	4.162542
238.430377	5922.674131	7.899776	-0.050169	4.165251
238.526838	5930.742449	7.904781	-0.050194	4.167976
238.633444	5938.734322	7.909786	-0.050220	4.170673
238.813429	5946.771701	7.914790	-0.050260	4.173386
238.874779	5954.811646	7.919795	-0.050278	4.176095
239.077191	5962.736503	7.924800	-0.050323	4.178766
239.512909	5970.845791	7.929805	-0.050411	4.181500
239.666825	5978.816071	7.934810	-0.050446	4.184182
240.109809	5986.840265	7.939814	-0.050535	4.186883
240.405491	5994.846440	7.944819	-0.050597	4.189576
240.289555	6002.909466	7.949824	-0.050582	4.192281
240.416652	6011.012234	7.954829	-0.050612	4.195000
240.899114	6018.969930	7.959834	-0.050708	4.197673
240.883603	6026.926282	7.964838	-0.050712	4.200338
241.169570	6034.953408	7.969843	-0.050772	4.203028
241.574405	6042.896436	7.974848	-0.050854	4.205690
241.854729	6050.971601	7.979853	-0.050913	4.208392
242.062309	6058.984090	7.984858	-0.050958	4.211072
242.034194	6067.008559	7.989862	-0.050959	4.213751
242.186179	6075.074166	7.994867	-0.050994	4.216444
242.505583	6083.001656	7.999872	-0.051060	4.219091
242.911868	6091.092055	8.004877	-0.051143	4.221791
243.074735	6098.997712	8.009882	-0.051179	4.224426
243.057962	6107.097272	8.014886	-0.051183	4.227121
243.244888	6115.097806	8.019891	-0.051224	4.229785
243.334813	6123.132431	8.024896	-0.051248	4.232456
243.811932	6131.179512	8.029901	-0.051343	4.235134
244.020575	6139.262658	8.034906	-0.051389	4.237820
244.423115	6147.187700	8.039910	-0.051470	4.240453
244.757366	6155.222321	8.044915	-0.051539	4.243120
244.943415	6163.196317	8.049920	-0.051580	4.245764
244.921244	6171.259100	8.054925	-0.051583	4.248434
245.220496	6179.262921	8.059930	-0.051645	4.251085
245.517454	6187.301203	8.064934	-0.051707	4.253746
245.874061	6195.370524	8.069939	-0.051780	4.256417
245.892329	6203.324145	8.074944	-0.051790	4.259044
246.124808	6211.386085	8.079949	-0.051840	4.261708
246.366136	6219.360183	8.084954	-0.051892	4.264340
246.174678	6227.390796	8.089958	-0.051863	4.266987
246.577567	6235.425901	8.094963	-0.051944	4.269637
246.703148	6243.453035	8.099968	-0.051974	4.272282
246.971686	6251.512108	8.104973	-0.052031	4.274936
247.205369	6259.522072	8.109978	-0.052081	4.277572
247.224273	6267.458590	8.114982	-0.052091	4.280181
247.315166	6275.516159	8.119987	-0.052115	4.282829
247.554230	6283.463027	8.124992	-0.052166	4.285439
247.982495	6291.516113	8.129997	-0.052252	4.288084
247.991294	6299.532593	8.135002	-0.052260	4.290713
248.107397	6307.603018	8.140006	-0.052289	4.293358
248.517458	6315.617455	8.145011	-0.052372	4.295986
248.479020	6323.634647	8.150016	-0.052371	4.298609
248.753616	6331.609655	8.155021	-0.052429	4.301219
248.915032	6339.593083	8.160026	-0.052465	4.303830
249.035936	6347.654025	8.165030	-0.052495	4.306464
249.060263	6355.650309	8.170035	-0.052506	4.309075
249.188188	6363.703797	8.175040	-0.052536	4.311703
249.389386	6371.751125	8.180045	-0.052580	4.314328
249.712715	6379.754867	8.185050	-0.052647	4.316939
249.987696	6387.694600	8.190054	-0.052705	4.319526
250.049861	6395.771243	8.195059	-0.052723	4.322155
250.225785	6403.718966	8.200064	-0.052762	4.324741
250.386254	6411.770798	8.205069	-0.052799	4.327360
250.629237	6419.788431	8.210074	-0.052851	4.329966
250.857101	6427.814191	8.215078	-0.052900	4.332573
251.007324	6435.874331	8.220083	-0.052934	4.335190
251.191583	6443.843403	8.225088	-0.052975	4.337775
251.465580	6451.869545	8.230093	-0.053033	4.340378
251.552721	6459.913843	8.235098	-0.053056	4.342984
251.575424	6467.872580	8.240102	-0.053067	4.345560
251.946915	6475.896137	8.245107	-0.053142	4.348158
251.993601	6483.926811	8.250112	-0.053158	4.350754
252.306659	6492.035720	8.255117	-0.053223	4.353376
252.504786	6500.069531	8.260122	-0.053266	4.355971
252.610920	6508.001490	8.265126	-0.053293	4.358532
252.698723	6516.006272	8.270131	-0.053316	4.361114
252.939923	6523.949205	8.275136	-0.053367	4.363676
253.127447	6532.003515	8.280141	-0.053409	4.366271
253.292766	6540.054356	8.285146	-0.053446	4.368864
253.558005	6548.053036	8.290150	-0.053502	4.371439
253.836470	6556.067983	8.295155	-0.053560	4.374018
254.247462	6564.085588	8.300160	-0.053644	4.376597
254.590046	6572.089770	8.305165	-0.053714	4.379169
254.774852	6580.156817	8.310170	-0.053755	4.381760
254.951472	6588.122740	8.315174	-0.053795	4.384316
255.058499	6596.188979	8.320179	-0.053821	4.386902
254.946140	6604.158186	8.325184	-0.053807	4.389455
255.153979	6612.231422	8.330189	-0.053852	4.392042
255.160769	6620.260847	8.335194	-0.053860	4.394611
255.158720	6628.270707	8.340198	-0.053866	4.397173
255.630102	6636.235257	8.345203	-0.053961	4.399721
255.864338	6644.266738	8.350208	-0.054011	4.402288
256.026204	6652.241455	8.355213	-0.054048	4.404835
256.230568	6660.326936	8.360218	-0.054092	4.407416
256.483077	6668.295146	8.365222	-0.054146	4.409958
256.916645	6676.382167	8.370227	-0.054233	4.412538
257.029872	6684.391208	8.375232	-0.054261	4.415089
257.137452	6692.463875	8.380237	-0.054288	4.417660
257.423957	6700.412309	8.385242	-0.054348	4.420190
257.440919	6708.454378	8.390246	-0.054357	4.422747
257.774548	6716.427285	8.395251	-0.054426	4.425282
257.957869	6724.447120	8.400256	-0.054467	4.427830
258.129973	6732.475734	8.405261	-0.054505	4.430379
258.356221	6740.566471	8.410266	-0.054554	4.432947
258.696086	6748.546372	8.415270	-0.054624	4.435478
258.934548	6756.560760	8.420275	-0.054675	4.438018
259.005572	6764.568976	8.425280	-0.054695	4.440555
259.264132	6772.537234	8.430285	-0.054750	4.443078
259.417045	6780.517247	8.435290	-0.054785	4.445602
259.409542	6788.565876	8.440294	-0.054790	4.448147
259.702341	6796.602022	8.445299	-0.054851	4.450687
259.729203	6804.637811	8.450304	-0.054863	4.453224
259.748282	6812.651568	8.455309	-0.054873	4.455754
260.022086	6820.658369	8.460314	-0.054931	4.458280
260.152361	6828.631651	8.465318	-0.054961	4.460794
260.420679	6836.686438	8.470323	-0.055018	4.463332
260.549200	6844.681821	8.475328	-0.055049	4.465850
260.657800	6852.732579	8.480333	-0.055075	4.468384
260.850967	6860.746465	8.485338	-0.055118	4.470905
260.974188	6868.751688	8.490342	-0.055148	4.473422
261.149991	6876.823638	8.495347	-0.055187	4.475958
261.450179	6884.769863	8.500352	-0.055249	4.478454
261.557738	6892.803893	8.505357	-0.055276	4.480975
261.732509	6900.804105	8.510362	-0.055315	4.483484
262.026719	6908.788980	8.515366	-0.055377	4.485988
262.275556	6916.855564	8.520371	-0.055430	4.488515
262.383453	6924.845102	8.525376	-0.055456	4.491017
262.646030	6932.900861	8.530381	-0.055512	4.493538
262.950001	6940.919017	8.535386	-0.055575	4.496047
262.932006	6948.881127	8.540390	-0.055578	4.498535
263.009773	6956.938960	8.545395	-0.055599	4.501053
263.338092	6964.901633	8.550400	-0.055667	4.503539
263.662947	6972.955943	8.555405	-0.055734	4.506053
263.700154	6980.962637	8.560410	-0.055748	4.508550
263.738020	6988.990824	8.565415	-0.055761	4.511052
264.119840	6997.109674	8.570419	-0.055839	4.513582
264.110578	7005.046907	8.575424	-0.055844	4.516053
264.371396	7013.051228	8.580429	-0.055899	4.518544
264.484554	7021.049824	8.585434	-0.055927	4.521032
264.555546	7028.999846	8.590439	-0.055947	4.523503
264.641660	7037.067779	8.595443	-0.055969	4.526009
264.839792	7045.055203	8.600448	-0.056013	4.528489
265.068120	7053.120426	8.605453	-0.056062	4.530992
265.182593	7061.162511	8.610458	-0.056090	4.533486
265.525418	7069.142638	8.615463	-0.056160	4.535960
265.878264	7077.156464	8.620467	-0.056233	4.538443
265.770542	7085.170515	8.625472	-0.056219	4.540924
265.989188	7093.187749	8.630477	-0.056267	4.543405
266.229361	7101.192224	8.635482	-0.056318	4.545881
266.313371	7109.165293	8.640487	-0.056340	4.548346
266.283868	7117.264375	8.645491	-0.056341	4.550848
266.597088	7125.297168	8.650496	-0.056406	4.553328
266.861788	7133.322458	8.655501	-0.056462	4.555805
266.813122	7141.327667	8.660506	-0.056460	4.558274
266.882109	7149.296425	8.665511	-0.056479	4.560730
267.358633	7157.348778	8.670515	-0.056574	4.563211
267.366172	7165.321366	8.675520	-0.056582	4.565666
267.490560	7173.359971	8.680525	-0.056612	4.568140
267.876786	7181.380287	8.685530	-0.056691	4.570607
267.984704	7189.423723	8.690535	-0.056718	4.573079
268.339215	7197.478430	8.695539	-0.056790	4.575554
268.440197	7205.467684	8.700544	-0.056816	4.578007
268.722089	7213.431653	8.705549	-0.056875	4.580452
268.733955	7221.492758	8.710554	-0.056883	4.582924
268.683015	7229.428880	8.715559	-0.056881	4.585357
269.103449	7237.526145	8.720563	-0.056966	4.587838
269.317506	7245.499448	8.725568	-0.057012	4.590280
269.581026	7253.562815	8.730573	-0.057068	4.592748
269.669353	7261.589701	8.735578	-0.057091	4.595203
269.757732	7269.587221	8.740583	-0.057114	4.597649
269.848641	7277.572694	8.745587	-0.057137	4.600089
270.087157	7285.601478	8.750592	-0.057188	4.602541
270.529890	7293.577631	8.755597	-0.057277	4.604975
270.605865	7301.668174	8.760602	-0.057298	4.607444
270.637816	7309.619638	8.765607	-0.057311	4.609868
271.016251	7317.710217	8.770611	-0.057388	4.612334
271.121026	7325.678595	8.775616	-0.057414	4.614761
271.282199	7333.701615	8.780621	-0.057451	4.617203
271.204480	7341.639063	8.785626	-0.057443	4.619618
271.409702	7349.689236	8.790631	-0.057488	4.622066
271.703848	7357.699848	8.795635	-0.057549	4.624501
271.747243	7365.750006	8.800640	-0.057564	4.626946
272.022458	7373.735278	8.805645	-0.057621	4.629370
272.285852	7381.789645	8.810650	-0.057677	4.631814
272.240284	7389.815317	8.815655	-0.057675	4.634248
272.578583	7397.890996	8.820659	-0.057745	4.636696
272.721432	7405.819802	8.825664	-0.057778	4.639098
272.791644	7413.827752	8.830669	-0.057798	4.641523
272.912433	7421.831900	8.835674	-0.057827	4.643945
273.081412	7429.884902	8.840679	-0.057865	4.646381
273.185503	7437.876819	8.845683	-0.057891	4.648797
273.291322	7445.898788	8.850688	-0.057917	4.651221
273.628667	7453.925183	8.855693	-0.057987	4.653645
273.866713	7461.983293	8.860698	-0.058038	4.656077
273.867275	7469.935691	8.865703	-0.058044	4.658476
274.205195	7477.962529	8.870707	-0.058114	4.660896
274.361785	7485.962533	8.875712	-0.058150	4.663307
274.389943	7493.942101	8.880717	-0.058161	4.665710
274.759387	7502.019286	8.885722	-0.058237	4.668141
274.981805	7510.006458	8.890727	-0.058285	4.670544
275.264169	7518.112467	8.895731	-0.058344	4.672982
275.310550	7526.132862	8.900736	-0.058359	4.675393
275.365511	7534.104479	8.905741	-0.058376	4.677788
275.494674	7542.066206	8.910746	-0.058407	4.680178
275.548783	7550.086636	8.915751	-0.058424	4.682585
275.760309	7558.094760	8.920755	-0.058470	4.684987
276.031619	7566.125274	8.925760	-0.058527	4.687394
276.151582	7574.066041	8.930765	-0.058556	4.689773
276.404192	7582.154855	8.935770	-0.058609	4.692195
276.540144	7590.153066	8.940775	-0.058641	4.694589
276.767931	7598.253299	8.945779	-0.058690	4.697012
276.825574	7606.154739	8.950784	-0.058708	4.699375
277.011411	7614.211818	8.955789	-0.058749	4.701783
277.489648	7622.216279	8.960794	-0.058844	4.704173
277.572379	7630.218069	8.965799	-0.058867	4.706561
277.762126	7638.265826	8.970803	-0.058908	4.708963
277.665604	7646.276175	8.975808	-0.058897	4.711352
278.015032	7654.330727	8.980813	-0.058969	4.713752
278.382218	7662.386573	8.985818	-0.059044	4.716152
278.359773	7670.310428	8.990823	-0.059046	4.718512
278.515624	7678.334593	8.995827	-0.059082	4.720900
278.507273	7686.355840	9.000832	-0.059087	4.723286
278.752163	7694.345127	9.005837	-0.059139	4.725661
279.196543	7702.426967	9.010842	-0.059229	4.728061
279.111020	7710.393429	9.015847	-0.059219	4.730428
279.558652	7718.459536	9.020851	-0.059309	4.732822
279.648662	7726.462491	9.025856	-0.059333	4.735196
279.778720	7734.475261	9.030861	-0.059363	4.737572
279.912763	7742.442655	9.035866	-0.059395	4.739934
279.837483	7750.491552	9.040871	-0.059388	4.742319
280.098754	7758.493946	9.045875	-0.059443	4.744688
280.120862	7766.480474	9.050880	-0.059453	4.747052
280.311744	7774.533384	9.055885	-0.059496	4.749434
280.747659	7782.586301	9.060890	-0.059583	4.751813
281.057142	7790.616365	9.065895	-0.059648	4.754185
281.188380	7798.636492	9.070899	-0.059679	4.756554
281.256784	7806.584710	9.075904	-0.059698	4.758901
281.348259	7814.573191	9.080909	-0.059722	4.761258
281.399545	7822.584157	9.085914	-0.059738	4.763620
281.545298	7830.574024	9.090919	-0.059772	4.765975
281.702956	7838.658162	9.095923	-0.059808	4.768357
281.780480	7846.680542	9.100928	-0.059829	4.770719
282.014670	7854.717794	9.105933	-0.059879	4.773084
282.243942	7862.745260	9.110938	-0.059928	4.775445
282.269993	7870.661088	9.115943	-0.059940	4.777773
282.498194	7878.755018	9.120947	-0.059989	4.780151
282.578774	7886.697667	9.125952	-0.060010	4.782484
282.883725	7894.705276	9.130957	-0.060074	4.784834
283.062191	7902.787239	9.135962	-0.060114	4.787205
283.063338	7910.737299	9.140967	-0.060120	4.789537
283.382027	7918.846717	9.145971	-0.060186	4.791913
283.403984	7926.824216	9.150976	-0.060197	4.794251
283.503904	7934.832547	9.155981	-0.060222	4.796596
283.694787	7942.825086	9.160986	-0.060264	4.798935
283.800267	7950.846795	9.165991	-0.060291	4.801282
283.977586	7958.889764	9.170995	-0.060330	4.803634
284.093640	7966.824567	9.176000	-0.060359	4.805953
284.414886	7974.906967	9.181005	-0.060425	4.808313
284.563594	7982.913334	9.186010	-0.060459	4.810650
284.561513	7990.363537	9.191015	-0.060465	4.812825
284.840876	7994.955467	9.196019	-0.060522	4.814163

284.918374	7997.468633	9.201024	-0.060539	4.814896
285.119848	7998.782520	9.206029	-0.060579	4.815278
285.096531	7999.230685	9.211034	-0.060576	4.815409
285.086000	8000.232486	9.216039	-0.060576	4.815701
285.220542	8000.227648	9.221043	-0.060603	4.815699
285.279330	8000.219253	9.226048	-0.060615	4.815696
285.385898	8000.250286	9.231053	-0.060636	4.815705
285.465610	8000.236931	9.236058	-0.060652	4.815700
285.660363	8000.222515	9.241063	-0.060690	4.815695
285.801727	8000.252059	9.246067	-0.060718	4.815703
285.841280	8000.252938	9.251072	-0.060727	4.815703
285.574194	8000.265210	9.256077	-0.060678	4.815708
285.847447	8000.240488	9.261082	-0.060731	4.815699
286.042222	8000.242129	9.266087	-0.060768	4.815698
285.995060	8000.264936	9.271091	-0.060761	4.815705
285.973253	8000.229344	9.276096	-0.060758	4.815695
286.127517	8000.255918	9.281101	-0.060788	4.815702
286.283114	8000.223644	9.286106	-0.060819	4.815691
286.255626	8000.239326	9.291111	-0.060815	4.815696
286.488450	8000.245962	9.296115	-0.060860	4.815697
286.456550	8000.212321	9.301120	-0.060855	4.815687
286.420941	8000.242838	9.306125	-0.060850	4.815696
286.444820	8000.245565	9.311130	-0.060856	4.815697
286.503575	8000.216832	9.316135	-0.060868	4.815688
286.689268	8000.231149	9.321139	-0.060904	4.815691
286.621396	8000.212892	9.326144	-0.060893	4.815686
286.648977	8000.243520	9.331149	-0.060899	4.815695
286.658748	8000.227786	9.336154	-0.060902	4.815690
286.736997	8000.250799	9.341159	-0.060918	4.815696
286.710235	8000.246156	9.346163	-0.060915	4.815695
286.793050	8000.222154	9.351168	-0.060932	4.815688
286.775176	8000.238016	9.356173	-0.060930	4.815692
286.790931	8000.234169	9.361178	-0.060934	4.815691
286.875040	8000.251939	9.366183	-0.060951	4.815696
286.891405	8000.283428	9.371187	-0.060956	4.815705
287.003003	8000.232133	9.376192	-0.060978	4.815689
287.179268	8000.267685	9.381197	-0.061012	4.815699
287.190226	8000.257325	9.386202	-0.061015	4.815695
287.048719	8000.251606	9.391207	-0.060990	4.815695
287.080046	8000.259825	9.396211	-0.060998	4.815697
287.118903	8000.235001	9.401216	-0.061006	4.815689
287.021215	8000.269708	9.406221	-0.060989	4.815700
287.051057	8000.260772	9.411226	-0.060996	4.815697
287.008719	8000.260120	9.416231	-0.060990	4.815697
287.132370	8000.260432	9.421235	-0.061014	4.815696
287.122498	8000.258246	9.426240	-0.061014	4.815696
287.280590	8000.276331	9.431245	-0.061045	4.815700
287.417396	8000.290806	9.436250	-0.061072	4.815704
287.316198	8000.280488	9.441255	-0.061054	4.815701
287.341002	8000.311065	9.446259	-0.061060	4.815710
287.299724	8000.277248	9.451264	-0.061054	4.815700
287.236017	8000.296535	9.456269	-0.061043	4.815706
287.353497	8000.293521	9.461274	-0.061067	4.815705
287.439179	8000.288841	9.466279	-0.061084	4.815703
287.651741	8000.305805	9.471283	-0.061125	4.815706
287.388267	8000.281745	9.476288	-0.061077	4.815701
287.455034	8000.306685	9.481293	-0.061091	4.815708
287.575512	8000.315502	9.486298	-0.061115	4.815710
287.592577	8000.289200	9.491303	-0.061119	4.815702
287.635251	8000.326534	9.496307	-0.061129	4.815712
287.659258	8000.315348	9.501312	-0.061135	4.815709
287.459995	8000.306406	9.506317	-0.061099	4.815707
287.660433	8000.307086	9.511322	-0.061138	4.815706
287.725067	8000.297731	9.516327	-0.061151	4.815703
287.840260	8000.326789	9.521331	-0.061174	4.815711
287.706672	8000.311583	9.526336	-0.061150	4.815707
287.734789	8000.324024	9.531341	-0.061157	4.815711
287.779783	8000.364614	9.536346	-0.061167	4.815722
287.728961	8000.332758	9.541351	-0.061159	4.815713
287.827307	8000.317611	9.546355	-0.061179	4.815708
287.859341	8000.310858	9.551360	-0.061186	4.815706
287.690833	8000.362437	9.556365	-0.061156	4.815722
287.704107	8000.356403	9.561370	-0.061160	4.815720
287.712576	8000.293543	9.566375	-0.061163	4.815702
287.812587	8000.304119	9.571379	-0.061183	4.815704
287.689915	8000.268778	9.576384	-0.061161	4.815695
287.772868	8000.310078	9.581389	-0.061178	4.815706
287.896119	8000.335005	9.586394	-0.061202	4.815713
287.983683	8000.308952	9.591399	-0.061220	4.815705
288.165880	8000.318925	9.596403	-0.061255	4.815706
288.026982	8000.286491	9.601408	-0.061231	4.815698
288.102057	8000.318010	9.606413	-0.061246	4.815706
288.061721	8000.314183	9.611418	-0.061240	4.815705
288.027415	8000.286919	9.616423	-0.061235	4.815698
288.093741	8000.325767	9.621427	-0.061249	4.815709
288.186147	8000.278395	9.626432	-0.061268	4.815694
288.015685	8000.319233	9.631437	-0.061237	4.815707
288.152431	8000.365824	9.636442	-0.061264	4.815720
287.901501	8000.343067	9.641447	-0.061219	4.815715
287.972385	8000.389495	9.646451	-0.061233	4.815728
287.992541	8000.348263	9.651456	-0.061239	4.815715
287.884809	8000.341033	9.656461	-0.061220	4.815714
288.158118	8000.322739	9.661466	-0.061272	4.815707
287.938800	8000.302716	9.666471	-0.061233	4.815702
288.306233	8000.346132	9.671475	-0.061302	4.815713
288.105713	8000.314684	9.676480	-0.061267	4.815705
288.106978	8000.334117	9.681485	-0.061268	4.815710
288.239263	8000.330310	9.686490	-0.061294	4.815709
288.058704	8000.291743	9.691495	-0.061262	4.815698
288.211700	8000.329003	9.696499	-0.061292	4.815708
288.096026	8000.262748	9.701504	-0.061272	4.815690
288.370162	8000.292642	9.706509	-0.061324	4.815697
288.161828	8000.308150	9.711514	-0.061287	4.815702
288.265042	8000.309152	9.716519	-0.061307	4.815702
288.366198	8000.366852	9.721523	-0.061328	4.815718
288.290052	8000.294913	9.726528	-0.061315	4.815698
288.241996	8000.303787	9.731533	-0.061307	4.815700
288.288393	8000.362603	9.736538	-0.061317	4.815717
288.103688	8000.303619	9.741543	-0.061284	4.815701
288.228635	8000.338213	9.746547	-0.061309	4.815710
288.311910	8000.294951	9.751552	-0.061326	4.815697
288.158592	8000.325406	9.756557	-0.061299	4.815707
288.312560	8000.339133	9.761562	-0.061329	4.815710
288.384601	8000.317071	9.766567	-0.061343	4.815703
288.437476	8000.358880	9.771571	-0.061355	4.815715
288.382257	8000.310884	9.776576	-0.061346	4.815701
288.493611	8000.306686	9.781581	-0.061368	4.815700
288.357991	8000.310710	9.786586	-0.061344	4.815701
288.259174	8000.279025	9.791591	-0.061327	4.815693
288.301230	8000.320631	9.796595	-0.061336	4.815705
288.327434	8000.295570	9.801600	-0.061343	4.815697
288.480609	8000.326411	9.806605	-0.061372	4.815705
288.295526	8000.330579	9.811610	-0.061339	4.815707
288.261073	8000.330074	9.816615	-0.061334	4.815707
288.325153	8000.366740	9.821619	-0.061348	4.815718
288.259048	8000.300341	9.826624	-0.061337	4.815699
288.305064	8000.340951	9.831629	-0.061347	4.815710
288.598144	8000.340157	9.836634	-0.061403	4.815708
288.446259	8000.297844	9.841639	-0.061376	4.815697
288.677860	8000.317308	9.846643	-0.061420	4.815701
288.620130	8000.298168	9.851648	-0.061411	4.815696
288.544320	8000.309734	9.856653	-0.061398	4.815700
288.635083	8000.327632	9.861658	-0.061417	4.815704
288.846748	8000.309255	9.866663	-0.061457	4.815698
288.766346	8000.345357	9.871667	-0.061444	4.815709
288.649146	8000.326174	9.876672	-0.061423	4.815704
288.355081	8000.336864	9.881677	-0.061370	4.815708
288.540602	8000.332985	9.886682	-0.061406	4.815706
288.750485	8000.329562	9.891687	-0.061446	4.815704
288.729453	8000.349648	9.896691	-0.061444	4.815710
288.788874	8000.302727	9.901696	-0.061456	4.815696
288.567344	8000.323340	9.906701	-0.061416	4.815703
288.667744	8000.334995	9.911706	-0.061437	4.815706
288.510549	8000.312922	9.916711	-0.061409	4.815700
288.687821	8000.367766	9.921715	-0.061443	4.815715
288.656969	8000.334142	9.926720	-0.061439	4.815705
288.775983	8000.326877	9.931725	-0.061462	4.815703
288.660561	8000.391227	9.936730	-0.061442	4.815722
288.696772	8000.343872	9.941735	-0.061450	4.815708
288.838802	8000.355236	9.946739	-0.061478	4.815710
288.768789	8000.357276	9.951744	-0.061467	4.815711
288.828854	8000.336060	9.956749	-0.061479	4.815705
288.769399	8000.375766	9.961754	-0.061469	4.815717
288.537379	8000.294483	9.966759	-0.061428	4.815694
288.682343	8000.328383	9.971763	-0.061456	4.815703
288.873900	8000.321406	9.976768	-0.061493	4.815700
288.558784	8000.335983	9.981773	-0.061436	4.815706
288.774966	8000.329467	9.986778	-0.061477	4.815703
288.710339	8000.327326	9.991783	-0.061467	4.815703
288.994732	8000.383108	9.996787	-0.061521	4.815717
288.728848	8000.336517	10.001792	-0.061473	4.815705
288.872723	8000.337211	10.006797	-0.061501	4.815705
288.816628	8000.359851	10.011802	-0.061492	4.815711
288.680331	8000.325323	10.016807	-0.061468	4.815702
288.776364	8000.334755	10.021811	-0.061487	4.815704
288.849953	8000.341626	10.026816	-0.061502	4.815706
288.896939	8000.322306	10.031821	-0.061513	4.815700
288.836316	8000.306323	10.036826	-0.061503	4.815695
288.942303	8000.300955	10.041831	-0.061524	4.815693
288.906720	8000.346461	10.046835	-0.061519	4.815707
288.667073	8000.311066	10.051840	-0.061475	4.815698
288.786328	8000.317722	10.056845	-0.061499	4.815699
288.889624	8000.347631	10.061850	-0.061520	4.815707
288.576829	8000.327995	10.066855	-0.061463	4.815703
288.717721	8000.320068	10.071859	-0.061490	4.815700
288.848405	8000.302316	10.076864	-0.061516	4.815694
288.934734	8000.322272	10.081869	-0.061534	4.815699
288.687108	8000.343466	10.086874	-0.061489	4.815707
288.866023	8000.340535	10.091879	-0.061524	4.815705
288.931971	8000.382590	10.096883	-0.061537	4.815717
288.888050	8000.347650	10.101888	-0.061530	4.815707
288.862545	8000.350524	10.106893	-0.061527	4.815708
289.165696	8000.391671	10.111898	-0.061585	4.815718
288.836902	8000.324631	10.116903	-0.061525	4.815700
288.851272	8000.372143	10.121907	-0.061529	4.815714
289.007789	8000.368792	10.126912	-0.061560	4.815712
288.876297	8000.353622	10.131917	-0.061537	4.815708
288.962839	8000.380006	10.136922	-0.061554	4.815715
288.874852	8000.345311	10.141927	-0.061539	4.815706
288.904596	8000.349220	10.146931	-0.061546	4.815707
288.840470	8000.353511	10.151936	-0.061535	4.815708
288.695139	8000.362704	10.156941	-0.061510	4.815712
288.826578	8000.361024	10.161946	-0.061536	4.815710
288.812761	8000.333072	10.166951	-0.061534	4.815702
288.781998	8000.393655	10.171955	-0.061530	4.815720
288.901219	8000.364984	10.176960	-0.061554	4.815711
288.924773	8000.385905	10.181965	-0.061560	4.815717
288.980916	8000.392449	10.186970	-0.061571	4.815719
288.826719	8000.314763	10.191975	-0.061544	4.815697
289.123773	8000.383630	10.196979	-0.061601	4.815715
288.809271	8000.335056	10.201984	-0.061544	4.815703
288.806367	8000.340495	10.206989	-0.061544	4.815704
289.007792	8000.358325	10.211994	-0.061583	4.815708
289.098170	8000.351594	10.216999	-0.061602	4.815706
289.070386	8000.384400	10.222003	-0.061598	4.815715
288.862681	8000.362449	10.227008	-0.061561	4.815710
288.901698	8000.344051	10.232013	-0.061569	4.815705
288.966987	8000.349696	10.237018	-0.061583	4.815706
288.984752	8000.318053	10.242023	-0.061587	4.815696
288.895481	8000.358271	10.247027	-0.061572	4.815709
288.858009	8000.344863	10.252032	-0.061567	4.815705
288.987491	8000.363486	10.257037	-0.061592	4.815710
289.182487	8000.376915	10.262042	-0.061630	4.815712
288.991315	8000.339216	10.267047	-0.061596	4.815702
288.987239	8000.364972	10.272051	-0.061596	4.815710
289.089421	8000.361674	10.277056	-0.061617	4.815708
289.090128	8000.353263	10.282061	-0.061618	4.815706
289.213850	8000.363215	10.287066	-0.061643	4.815708
289.133340	8000.347929	10.292071	-0.061629	4.815704
289.149821	8000.376212	10.297075	-0.061633	4.815712
289.187795	8000.341736	10.302080	-0.061642	4.815702
289.029601	8000.365675	10.307085	-0.061614	4.815710
289.206671	8000.433366	10.312090	-0.061648	4.815728
289.163061	8000.384514	10.317095	-0.061641	4.815714
289.206195	8000.440060	10.322099	-0.061651	4.815730
288.909166	8000.361837	10.327104	-0.061597	4.815709
289.192894	8000.353376	10.332109	-0.061651	4.815705
289.210490	8000.362410	10.337114	-0.061656	4.815707
289.239052	8000.359874	10.342119	-0.061663	4.815706
289.332491	8000.369259	10.347123	-0.061681	4.815709
289.321428	8000.377756	10.352128	-0.061681	4.815711
289.013786	8000.360355	10.357133	-0.061625	4.815708
289.098401	8000.398479	10.362138	-0.061642	4.815718
289.105380	8000.371986	10.367143	-0.061645	4.815710
289.148615	8000.391136	10.372147	-0.061654	4.815716
289.213987	8000.380725	10.377152	-0.061668	4.815712
289.059977	8000.391896	10.382157	-0.061640	4.815716
289.054363	8000.437964	10.387162	-0.061641	4.815730
289.045867	8000.371571	10.392167	-0.061641	4.815710
289.344688	8000.384804	10.397171	-0.061698	4.815713
289.199113	8000.418615	10.402176	-0.061672	4.815723
289.152880	8000.385772	10.407181	-0.061665	4.815714
289.300666	8000.414375	10.412186	-0.061694	4.815721
289.022076	8000.330074	10.417191	-0.061643	4.815698
289.300418	8000.370758	10.422195	-0.061696	4.815709
289.134178	8000.358147	10.427200	-0.061667	4.815706
289.194445	8000.369052	10.432205	-0.061679	4.815709
289.321000	8000.392974	10.437210	-0.061704	4.815715
289.280586	8000.351676	10.442215	-0.061698	4.815703
289.302168	8000.389690	10.447219	-0.061704	4.815714
289.211030	8000.409533	10.452224	-0.061688	4.815720
289.106599	8000.357400	10.457229	-0.061670	4.815705
289.451342	8000.416458	10.462234	-0.061736	4.815721
289.321684	8000.371345	10.467239	-0.061713	4.815708
289.350653	8000.372028	10.472243	-0.061720	4.815708
289.371453	8000.401463	10.477248	-0.061725	4.815717
289.541064	8000.391935	10.482253	-0.061758	4.815713
289.456157	8000.450435	10.487258	-0.061743	4.815730
289.216417	8000.366861	10.492263	-0.061700	4.815707
289.428792	8000.429862	10.497267	-0.061741	4.815724
289.448271	8000.372557	10.502272	-0.061746	4.815708
289.295537	8000.363411	10.507277	-0.061719	4.815706
289.479175	8000.388404	10.512282	-0.061755	4.815712
289.367349	8000.353261	10.517287	-0.061735	4.815702
289.463194	8000.401231	10.522291	-0.061754	4.815716
289.356712	8000.403657	10.527296	-0.061736	4.815717
289.237791	8000.382299	10.532301	-0.061715	4.815711
289.501762	8000.412009	10.537306	-0.061766	4.815719
289.478855	8000.353909	10.542311	-0.061763	4.815702
289.339305	8000.387833	10.547315	-0.061738	4.815712
289.239155	8000.385025	10.552320	-0.061721	4.815712
289.121611	8000.374398	10.557325	-0.061701	4.815710
289.256283	8000.466989	10.562330	-0.061727	4.815736
289.334839	8000.402226	10.567335	-0.061743	4.815716
289.235378	8000.412278	10.572339	-0.061726	4.815720
289.239124	8000.381443	10.577344	-0.061728	4.815711
289.440628	8000.376795	10.582349	-0.061767	4.815708
289.524771	8000.437393	10.587354	-0.061784	4.815725
289.297339	8000.422564	10.592359	-0.061743	4.815722
289.189413	8000.396059	10.597363	-0.061724	4.815715
289.294491	8000.358557	10.602368	-0.061745	4.815704
289.344885	8000.383194	10.607373	-0.061756	4.815710
289.508868	8000.402466	10.612378	-0.061788	4.815715
289.486964	8000.387208	10.617383	-0.061785	4.815711
289.296275	8000.428737	10.622387	-0.061751	4.815724
289.075636	8000.366932	10.627392	-0.061711	4.815707
289.135154	8000.397092	10.632397	-0.061724	4.815715
289.369542	8000.413402	10.637402	-0.061769	4.815719
289.116527	8000.409870	10.642407	-0.061723	4.815719
289.227971	8000.432439	10.647411	-0.061745	4.815725
289.267232	8000.404410	10.652416	-0.061754	4.815717
289.236286	8000.390053	10.657421	-0.061750	4.815713
289.277852	8000.429512	10.662426	-0.061759	4.815724
289.348115	8000.353888	10.667431	-0.061773	4.815701
289.366131	8000.430376	10.672435	-0.061778	4.815724
289.210717	8000.408333	10.677440	-0.061751	4.815718
289.373869	8000.387979	10.682445	-0.061782	4.815711
289.491151	8000.404234	10.687450	-0.061806	4.815715
289.377458	8000.393679	10.692455	-0.061786	4.815713
289.321891	8000.392777	10.697459	-0.061777	4.815713
289.367386	8000.417323	10.702464	-0.061787	4.815720
289.252574	8000.404605	10.707469	-0.061767	4.815716
289.142716	8000.405898	10.712474	-0.061748	4.815717
289.150822	8000.364438	10.717479	-0.061750	4.815705
289.362195	8000.392092	10.722483	-0.061791	4.815712
289.207107	8000.396819	10.727488	-0.061764	4.815714
289.252726	8000.363556	10.732493	-0.061774	4.815704
289.368107	8000.384058	10.737498	-0.061796	4.815710
289.192784	8000.369136	10.742503	-0.061765	4.815706
289.235563	8000.369007	10.747507	-0.061775	4.815706
289.518957	8000.365894	10.752512	-0.061829	4.815703
289.420346	8000.357763	10.757517	-0.061812	4.815701
289.365594	8000.393276	10.762522	-0.061803	4.815712
289.381754	8000.371237	10.767527	-0.061807	4.815705
289.396577	8000.379148	10.772531	-0.061812	4.815708
289.264680	8000.419639	10.777536	-0.061788	4.815720
289.254905	8000.397114	10.782541	-0.061788	4.815714
289.561379	8000.409422	10.787546	-0.061846	4.815715
289.397833	8000.375450	10.792551	-0.061817	4.815706
289.452774	8000.418372	10.797555	-0.061829	4.815719
289.521170	8000.397312	10.802560	-0.061843	4.815712
289.437950	8000.385186	10.807565	-0.061829	4.815709
289.383472	8000.409999	10.812570	-0.061820	4.815716
289.138586	8000.344527	10.817575	-0.061776	4.815699
289.373813	8000.398322	10.822579	-0.061821	4.815713
289.489295	8000.367439	10.827584	-0.061844	4.815703
289.335150	8000.394665	10.832589	-0.061817	4.815712
289.458112	8000.412098	10.837594	-0.061841	4.815716
289.407444	8000.358831	10.842599	-0.061833	4.815701
289.339007	8000.412287	10.847603	-0.061822	4.815717
289.372228	8000.388426	10.852608	-0.061829	4.815710
289.394906	8000.420038	10.857613	-0.061835	4.815719
289.568638	8000.468400	10.862618	-0.061869	4.815732
289.505897	8000.428822	10.867623	-0.061858	4.815721
289.472896	8000.410144	10.872627	-0.061854	4.815715
289.499190	8000.411848	10.877632	-0.061860	4.815716
289.231494	8000.448722	10.882637	-0.061811	4.815728
289.357383	8000.438375	10.887642	-0.061836	4.815724
289.462143	8000.401938	10.892647	-0.061857	4.815713
289.551979	8000.438021	10.897651	-0.061875	4.815723
289.542892	8000.420861	10.902656	-0.061875	4.815718
289.526272	8000.415337	10.907661	-0.061873	4.815716
289.580106	8000.400427	10.912666	-0.061885	4.815712
289.408316	8000.349171	10.917671	-0.061854	4.815698
289.572512	8000.397353	10.922675	-0.061886	4.815711
289.428138	8000.364811	10.927680	-0.061861	4.815702
289.373821	8000.381062	10.932685	-0.061852	4.815707
289.582611	8000.465409	10.937690	-0.061892	4.815730
289.371234	8000.421975	10.942695	-0.061854	4.815719
289.294141	8000.403541	10.947699	-0.061841	4.815714
289.326356	8000.375379	10.952704	-0.061849	4.815705
289.156279	8000.380896	10.957709	-0.061818	4.815708
289.497000	8000.391705	10.962714	-0.061883	4.815709
289.361780	8000.363616	10.967719	-0.061859	4.815702
289.349740	8000.389225	10.972723	-0.061858	4.815709
289.259639	8000.382323	10.977728	-0.061843	4.815708
289.183346	8000.359621	10.982733	-0.061830	4.815701
289.470105	8000.435795	10.987738	-0.061885	4.815722
289.441192	8000.357241	10.992743	-0.061881	4.815699
289.534904	8000.393396	10.997747	-0.061900	4.815709
289.555255	8000.401412	11.002752	-0.061905	4.815711
289.506057	8000.377077	11.007757	-0.061897	4.815705
289.574374	8000.400980	11.012762	-0.061911	4.815711
289.388801	8000.365523	11.017767	-0.061878	4.815702
289.365212	8000.404832	11.022771	-0.061875	4.815713
289.531433	8000.383465	11.027776	-0.061908	4.815706
289.353816	8000.395264	11.032781	-0.061876	4.815710
289.601482	8000.412894	11.037786	-0.061923	4.815714
289.597148	8000.377624	11.042791	-0.061924	4.815704
289.343729	8000.444741	11.047795	-0.061878	4.815725
289.134437	8000.412052	11.052800	-0.061841	4.815716
289.323385	8000.379335	11.057805	-0.061877	4.815706
289.503153	8000.447080	11.062810	-0.061912	4.815724
289.303939	8000.371756	11.067815	-0.061876	4.815704
289.490148	8000.388234	11.072819	-0.061912	4.815707
289.722736	8000.417359	11.077824	-0.061957	4.815715
289.626265	8000.373937	11.082829	-0.061941	4.815702
289.733686	8000.400715	11.087834	-0.061962	4.815710
289.770919	8000.368365	11.092839	-0.061970	4.815700
289.649718	8000.384432	11.097843	-0.061949	4.815705
289.674249	8000.373256	11.102848	-0.061955	4.815702
289.689158	8000.386522	11.107853	-0.061959	4.815705
289.771775	8000.404270	11.112858	-0.061976	4.815710
289.490542	8000.378796	11.117863	-0.061925	4.815704
289.478761	8000.442951	11.122867	-0.061924	4.815723
289.756228	8000.479341	11.127872	-0.061977	4.815732
289.370535	8000.433707	11.132877	-0.061907	4.815721
289.298370	8000.459259	11.137882	-0.061895	4.815729
289.414032	8000.436944	11.142887	-0.061918	4.815721
289.808429	8000.456256	11.147891	-0.061993	4.815725
289.725022	8000.422714	11.152896	-0.061978	4.815715
289.502616	8000.446519	11.157901	-0.061938	4.815724
289.795805	8000.444663	11.162906	-0.061994	4.815721
289.376262	8000.421948	11.167911	-0.061918	4.815717
289.465547	8000.458021	11.172915	-0.061936	4.815727
289.579588	8000.442100	11.177920	-0.061958	4.815722
289.404984	8000.416483	11.182925	-0.061927	4.815715
289.690744	8000.411276	11.187930	-0.061982	4.815712
289.532539	8000.430932	11.192935	-0.061954	4.815719
289.371171	8000.433399	11.197939	-0.061925	4.815720
289.388775	8000.425304	11.202944	-0.061930	4.815718
289.418478	8000.403519	11.207949	-0.061937	4.815711
289.530004	8000.440009	11.212954	-0.061959	4.815721
289.445426	8000.411799	11.217959	-0.061944	4.815713
289.544722	8000.402024	11.222963	-0.061964	4.815710
289.694398	8000.399618	11.227968	-0.061994	4.815708
289.382112	8000.384267	11.232973	-0.061937	4.815705
289.519992	8000.398769	11.237978	-0.061964	4.815709
289.571082	8000.426632	11.242983	-0.061975	4.815717
289.802592	8000.441819	11.247987	-0.062019	4.815720
289.746629	8000.426992	11.252992	-0.062010	4.815716
289.672432	8000.374352	11.257997	-0.061998	4.815701
289.793797	8000.444216	11.263002	-0.062022	4.815720
289.629043	8000.418783	11.268007	-0.061993	4.815714
289.492262	8000.424923	11.273011	-0.061968	4.815716
289.603639	8000.444282	11.278016	-0.061991	4.815721
289.529951	8000.425910	11.283021	-0.061978	4.815716
289.396127	8000.448165	11.288026	-0.061955	4.815724
289.421635	8000.427371	11.293031	-0.061961	4.815717
289.434740	8000.469510	11.298035	-0.061965	4.815729
289.217940	8000.500914	11.303040	-0.061926	4.815740
289.334497	8000.425087	11.308045	-0.061949	4.815717
289.570067	8000.440350	11.313050	-0.061994	4.815720
289.560764	8000.410339	11.318055	-0.061994	4.815711
289.534993	8000.421772	11.323059	-0.061990	4.815715
289.594841	8000.432670	11.328064	-0.062003	4.815718
289.381847	8000.409546	11.333069	-0.061965	4.815712
289.416030	8000.432809	11.338074	-0.061972	4.815719
289.445879	8000.399250	11.343079	-0.061979	4.815709
289.605461	8000.425936	11.348083	-0.062010	4.815715
289.581244	8000.420268	11.353088	-0.062007	4.815714
289.584926	8000.437607	11.358093	-0.062009	4.815719
289.690865	8000.446158	11.363098	-0.062031	4.815721
289.401126	8000.388405	11.368103	-0.061978	4.815705
289.435462	8000.382766	11.373107	-0.061986	4.815704
289.682152	8000.402520	11.378112	-0.062033	4.815708
289.614399	8000.387472	11.383117	-0.062022	4.815704
289.569008	8000.443502	11.388122	-0.062015	4.815720
289.378689	8000.409026	11.393127	-0.061981	4.815711
289.464112	8000.410768	11.398131	-0.061998	4.815711
289.464378	8000.401278	11.403136	-0.061999	4.815709
289.461477	8000.390657	11.408141	-0.062000	4.815705
289.906359	8000.409847	11.413146	-0.062085	4.815709
289.774197	8000.406437	11.418151	-0.062061	4.815708
289.635799	8000.447877	11.423155	-0.062037	4.815721
289.559395	8000.472278	11.428160	-0.062024	4.815729
289.760281	8000.449421	11.433165	-0.062063	4.815721
289.781471	8000.427476	11.438170	-0.062068	4.815714
289.534429	8000.401571	11.443175	-0.062024	4.815708
289.586238	8000.396259	11.448179	-0.062035	4.815706
289.539896	8000.394459	11.453184	-0.062027	4.815706
289.503037	8000.385343	11.458189	-0.062022	4.815703
289.665321	8000.403515	11.463194	-0.062054	4.815708
289.624222	8000.385755	11.468199	-0.062047	4.815703
289.529382	8000.392681	11.473203	-0.062031	4.815705
289.489982	8000.413494	11.478208	-0.062025	4.815711
289.808466	8000.385348	11.483213	-0.062086	4.815701
289.649074	8000.437100	11.488218	-0.062057	4.815717
289.464545	8000.380249	11.493223	-0.062024	4.815702
289.582796	8000.389030	11.498227	-0.062048	4.815704
289.649208	8000.388275	11.503232	-0.062062	4.815703
289.631547	8000.395578	11.508237	-0.062060	4.815705
289.798419	8000.435248	11.513242	-0.062092	4.815716
289.764865	8000.410135	11.518247	-0.062087	4.815709
289.480601	8000.419932	11.523251	-0.062036	4.815713
289.604268	8000.453439	11.528256	-0.062060	4.815722
289.709245	8000.392382	11.533261	-0.062081	4.815704
289.577008	8000.432867	11.538266	-0.062058	4.815716
289.592194	8000.396891	11.543271	-0.062062	4.815705
289.657371	8000.389689	11.548275	-0.062076	4.815703
289.542487	8000.397310	11.553280	-0.062056	4.815706
289.617825	8000.353897	11.558285	-0.062071	4.815693
289.921615	8000.399347	11.563290	-0.062129	4.815704
289.778821	8000.387174	11.568295	-0.062104	4.815701
289.838107	8000.393779	11.573299	-0.062116	4.815703
289.859027	8000.403947	11.578304	-0.062122	4.815706
289.654753	8000.389550	11.583309	-0.062085	4.815703
289.671657	8000.416772	11.588314	-0.062089	4.815710
289.536217	8000.354418	11.593319	-0.062066	4.815693
289.955077	8000.405238	11.598323	-0.062145	4.815705
289.920341	8000.358691	11.603328	-0.062140	4.815692
289.752240	8000.383514	11.608333	-0.062110	4.815700
289.820946	8000.430979	11.613338	-0.062124	4.815714
289.831462	8000.359585	11.618343	-0.062128	4.815693
289.741963	8000.397659	11.623347	-0.062112	4.815704
289.906851	8000.435152	11.628352	-0.062144	4.815714
289.777960	8000.447863	11.633357	-0.062122	4.815719
289.867799	8000.475383	11.638362	-0.062140	4.815726
289.734424	8000.436620	11.643367	-0.062116	4.815715
289.691323	8000.429528	11.648371	-0.062110	4.815714
289.832122	8000.418391	11.653376	-0.062137	4.815710
289.650198	8000.380860	11.658381	-0.062105	4.815700
289.724192	8000.422000	11.663386	-0.062120	4.815711
289.802313	8000.406476	11.668391	-0.062136	4.815706
289.738738	8000.418271	11.673395	-0.062126	4.815710
289.680106	8000.424805	11.678400	-0.062116	4.815712
289.888005	8000.396727	11.683405	-0.062156	4.815703
289.727360	8000.349959	11.688410	-0.062128	4.815690
289.760978	8000.355012	11.693415	-0.062135	4.815691
289.817786	8000.395830	11.698419	-0.062147	4.815703
290.022288	8000.358052	11.703424	-0.062187	4.815690
289.655962	8000.385581	11.708429	-0.062120	4.815700
289.663951	8000.414777	11.713434	-0.062123	4.815709
289.675369	8000.392649	11.718439	-0.062126	4.815702
289.701232	8000.427533	11.723443	-0.062133	4.815712
289.658846	8000.395831	11.728448	-0.062126	4.815703
289.587613	8000.394635	11.733453	-0.062114	4.815703
289.627671	8000.423362	11.738458	-0.062123	4.815711
289.623087	8000.399863	11.743463	-0.062124	4.815705
289.528221	8000.414283	11.748467	-0.062107	4.815709
289.779854	8000.421284	11.753472	-0.062156	4.815710
289.644848	8000.377138	11.758477	-0.062132	4.815698
289.763866	8000.406276	11.763482	-0.062155	4.815705
289.819552	8000.393542	11.768487	-0.062167	4.815701
289.875796	8000.408656	11.773491	-0.062179	4.815705
289.634364	8000.396773	11.778496	-0.062135	4.815703
289.792187	8000.402014	11.783501	-0.062166	4.815704
289.797209	8000.448285	11.788506	-0.062169	4.815717
289.656020	8000.411517	11.793511	-0.062144	4.815707
289.609233	8000.409709	11.798515	-0.062136	4.815707
289.602508	8000.443983	11.803520	-0.062136	4.815717
289.426391	8000.416195	11.808525	-0.062105	4.815710
289.600074	8000.441005	11.813530	-0.062139	4.815716
289.788480	8000.428621	11.818535	-0.062175	4.815711
289.805193	8000.413015	11.823539	-0.062180	4.815707
289.747576	8000.406721	11.828544	-0.062170	4.815705
289.736674	8000.384174	11.833549	-0.062170	4.815699
289.981032	8000.403887	11.838554	-0.062217	4.815703
289.827168	8000.373304	11.843559	-0.062189	4.815695
289.649049	8000.393657	11.848563	-0.062158	4.815702
289.853715	8000.391212	11.853568	-0.062197	4.815700
289.796947	8000.396711	11.858573	-0.062188	4.815702
289.796602	8000.419328	11.863578	-0.062189	4.815708
289.720086	8000.385914	11.868583	-0.062176	4.815699
289.825987	8000.405171	11.873587	-0.062198	4.815704
289.797107	8000.399416	11.878592	-0.062194	4.815702
289.630032	8000.385716	11.883597	-0.062164	4.815699
289.592016	8000.452592	11.888602	-0.062158	4.815719
289.521854	8000.392532	11.893607	-0.062146	4.815702
289.666246	8000.387886	11.898611	-0.062175	4.815700
289.907558	8000.424672	11.903616	-0.062221	4.815709
289.818620	8000.407084	11.908621	-0.062206	4.815704
289.944359	8000.439561	11.913626	-0.062231	4.815713
289.884642	8000.419309	11.918631	-0.062221	4.815707
289.949808	8000.415319	11.923635	-0.062234	4.815706
289.741088	8000.421179	11.928640	-0.062197	4.815709
289.672602	8000.413611	11.933645	-0.062186	4.815707
290.040833	8000.453848	11.938650	-0.062256	4.815716
289.702791	8000.446576	11.943655	-0.062194	4.815716
289.773567	8000.411643	11.948659	-0.062209	4.815705
289.880011	8000.470523	11.953664	-0.062230	4.815722
289.637026	8000.400796	11.958669	-0.062186	4.815703
289.637306	8000.424495	11.963674	-0.062187	4.815710
289.725566	8000.371690	11.968679	-0.062205	4.815694
289.720719	8000.415634	11.973683	-0.062206	4.815707
289.962147	8000.419233	11.978688	-0.062252	4.815706
289.637863	8000.396160	11.983693	-0.062193	4.815701
289.688568	8000.444358	11.988698	-0.062204	4.815715
289.581337	8000.406086	11.993703	-0.062185	4.815705
289.584181	8000.408420	11.998707	-0.062187	4.815705
289.664492	8000.396149	12.003712	-0.062204	4.815701
289.757752	8000.381979	12.008717	-0.062222	4.815696
289.802259	8000.426850	12.013722	-0.062232	4.815709
289.623980	8000.388315	12.018727	-0.062200	4.815699
289.717595	8000.399847	12.023731	-0.062219	4.815702
289.782716	8000.416198	12.028736	-0.062233	4.815706
289.535876	8000.414919	12.033741	-0.062188	4.815707
289.812085	8000.443795	12.038746	-0.062241	4.815714
289.800903	8000.411606	12.043751	-0.062240	4.815705
289.827077	8000.425085	12.048755	-0.062246	4.815708
289.920381	8000.435541	12.053760	-0.062265	4.815711
289.816598	8000.385555	12.058765	-0.062247	4.815697
289.779873	8000.442820	12.063770	-0.062242	4.815714
289.836855	8000.396922	12.068775	-0.062254	4.815700
290.016447	8000.417562	12.073779	-0.062289	4.815705
289.970307	8000.440390	12.078784	-0.062281	4.815712
289.807207	8000.391433	12.083789	-0.062252	4.815698
290.073603	8000.454386	12.088794	-0.062303	4.815715
290.089983	8000.451621	12.093799	-0.062308	4.815714
289.977798	8000.444303	12.098803	-0.062288	4.815713
290.148862	8000.416605	12.103808	-0.062322	4.815704
290.012852	8000.427041	12.108813	-0.062298	4.815707
290.071555	8000.435777	12.113818	-0.062310	4.815710
290.030972	8000.420166	12.118823	-0.062304	4.815705
289.887093	8000.411183	12.123827	-0.062278	4.815703
289.951536	8000.388979	12.128832	-0.062292	4.815696
289.788252	8000.384985	12.133837	-0.062263	4.815696
289.927846	8000.448770	12.138842	-0.062290	4.815714
289.891425	8000.404331	12.143847	-0.062285	4.815701
289.817805	8000.426643	12.148851	-0.062273	4.815708
289.902644	8000.430517	12.153856	-0.062290	4.815709
290.134012	8000.418939	12.158861	-0.062334	4.815704
289.959558	8000.432936	12.163866	-0.062303	4.815709
289.924263	8000.403506	12.168871	-0.062298	4.815700
289.959651	8000.426794	12.173875	-0.062306	4.815707
289.985181	8000.444543	12.178880	-0.062312	4.815712
289.827357	8000.414956	12.183885	-0.062284	4.815704
290.007997	8000.465594	12.188890	-0.062319	4.815718
289.909105	8000.402852	12.193895	-0.062302	4.815700
289.971011	8000.424496	12.198899	-0.062315	4.815706
289.859342	8000.419329	12.203904	-0.062296	4.815705
289.805508	8000.402399	12.208909	-0.062287	4.815700
289.817004	8000.425239	12.213914	-0.062290	4.815707
289.634260	8000.404820	12.218919	-0.062258	4.815702
289.878412	8000.430954	12.223923	-0.062305	4.815708
289.934775	8000.426798	12.228928	-0.062317	4.815707
289.863947	8000.399914	12.233933	-0.062305	4.815699
290.084657	8000.439527	12.238938	-0.062347	4.815710
289.959542	8000.398776	12.243943	-0.062325	4.815698
289.947090	8000.429731	12.248947	-0.062324	4.815707
289.964919	8000.447336	12.253952	-0.062329	4.815712
289.880259	8000.397709	12.258957	-0.062315	4.815698
289.882829	8000.395756	12.263962	-0.062317	4.815698
289.715085	8000.401314	12.268967	-0.062287	4.815700
289.799194	8000.404103	12.273971	-0.062304	4.815700
290.033399	8000.450393	12.278976	-0.062349	4.815713
289.910278	8000.416103	12.283981	-0.062327	4.815703
289.844147	8000.424638	12.288986	-0.062316	4.815706
289.857252	8000.391835	12.293991	-0.062320	4.815696
289.646137	8000.408356	12.298995	-0.062282	4.815702
289.753607	8000.421219	12.304000	-0.062304	4.815705
289.798728	8000.387945	12.309005	-0.062313	4.815695
289.902193	8000.392168	12.314010	-0.062334	4.815696
289.893896	8000.388941	12.319015	-0.062334	4.815695
289.956543	8000.385974	12.324019	-0.062347	4.815694
289.831304	8000.448002	12.329024	-0.062325	4.815713
289.864499	8000.416646	12.334029	-0.062333	4.815703
289.744252	8000.444508	12.339034	-0.062312	4.815712
289.730207	8000.429396	12.344039	-0.062310	4.815708
289.835899	8000.426166	12.349043	-0.062332	4.815706
289.738582	8000.444822	12.354048	-0.062315	4.815712
289.838447	8000.392233	12.359053	-0.062335	4.815696
290.060096	8000.410451	12.364058	-0.062377	4.815700
290.007695	8000.388195	12.369063	-0.062369	4.815694
289.965982	8000.418601	12.374067	-0.062363	4.815703
289.949612	8000.468755	12.379072	-0.062361	4.815718
289.749792	8000.454439	12.384077	-0.062325	4.815715
289.823928	8000.469888	12.389082	-0.062340	4.815719
289.759585	8000.453832	12.394087	-0.062330	4.815714
289.790860	8000.462054	12.399091	-0.062337	4.815716
289.845611	8000.447162	12.404096	-0.062349	4.815712
289.738242	8000.403532	12.409101	-0.062330	4.815700
289.848428	8000.456060	12.414106	-0.062352	4.815714
289.711285	8000.461121	12.419111	-0.062328	4.815716
289.725378	8000.422983	12.424115	-0.062332	4.815705
289.879227	8000.463482	12.429120	-0.062362	4.815716
290.006247	8000.429604	12.434125	-0.062387	4.815705
290.007818	8000.458682	12.439130	-0.062389	4.815714
289.897451	8000.463174	12.444135	-0.062369	4.815716
289.848583	8000.457044	12.449139	-0.062362	4.815714
289.963818	8000.459347	12.454144	-0.062385	4.815714
289.789981	8000.401622	12.459149	-0.062354	4.815698
289.945158	8000.429299	12.464154	-0.062384	4.815705
289.821139	8000.389639	12.469159	-0.062362	4.815695
289.979801	8000.417382	12.474163	-0.062393	4.815702
290.000398	8000.429686	12.479168	-0.062398	4.815705
289.914664	8000.417510	12.484173	-0.062384	4.815702
289.910045	8000.448613	12.489178	-0.062384	4.815711
289.998459	8000.419363	12.494183	-0.062402	4.815702
289.843056	8000.431576	12.499187	-0.062375	4.815706
289.930740	8000.438715	12.504192	-0.062392	4.815708
289.835762	8000.417801	12.509197	-0.062376	4.815702
290.008379	8000.447947	12.514202	-0.062410	4.815710
290.024834	8000.431266	12.519207	-0.062414	4.815705
289.996444	8000.420167	12.524211	-0.062410	4.815702
290.040951	8000.450050	12.529216	-0.062420	4.815710
290.081627	8000.414551	12.534221	-0.062429	4.815700
290.011977	8000.455140	12.539226	-0.062417	4.815712
289.801338	8000.395653	12.544231	-0.062379	4.815696
289.839259	8000.421130	12.549235	-0.062388	4.815703
289.839768	8000.416997	12.554240	-0.062389	4.815702
290.001483	8000.410536	12.559245	-0.062421	4.815699
290.012414	8000.415164	12.564250	-0.062424	4.815700
289.902440	8000.389686	12.569255	-0.062405	4.815693
289.991636	8000.406489	12.574259	-0.062423	4.815698
290.290636	8000.428301	12.579264	-0.062480	4.815702
290.144223	8000.402139	12.584269	-0.062454	4.815695
290.047149	8000.463626	12.589274	-0.062438	4.815714
289.842942	8000.422461	12.594279	-0.062401	4.815703
289.826779	8000.436216	12.599283	-0.062399	4.815707
290.053671	8000.430979	12.604288	-0.062443	4.815704
289.885346	8000.392628	12.609293	-0.062413	4.815694
289.966166	8000.414627	12.614298	-0.062429	4.815700
289.823829	8000.429227	12.619303	-0.062404	4.815705
289.849097	8000.409499	12.624307	-0.062410	4.815699
290.098058	8000.461421	12.629312	-0.062458	4.815713
290.150043	8000.398297	12.634317	-0.062469	4.815694
290.261708	8000.447642	12.639322	-0.062491	4.815708
290.242565	8000.436716	12.644327	-0.062489	4.815705
290.246359	8000.451917	12.649331	-0.062491	4.815709
290.279820	8000.464463	12.654336	-0.062499	4.815712
290.277305	8000.448496	12.659341	-0.062500	4.815708
290.199620	8000.486792	12.664346	-0.062487	4.815719
290.311722	8000.470836	12.669351	-0.062509	4.815714
290.115626	8000.433034	12.674355	-0.062474	4.815704
290.157660	8000.451094	12.679360	-0.062483	4.815709
290.116224	8000.417265	12.684365	-0.062477	4.815699
290.202485	8000.441509	12.689370	-0.062494	4.815706
290.230878	8000.434687	12.694375	-0.062501	4.815704
290.193035	8000.444824	12.699379	-0.062495	4.815707
290.125496	8000.451191	12.704384	-0.062484	4.815709
289.947677	8000.385895	12.709389	-0.062452	4.815691
290.321113	8000.435871	12.714394	-0.062523	4.815703
290.234073	8000.415106	12.719399	-0.062509	4.815698
290.109014	8000.425747	12.724403	-0.062487	4.815701
290.076429	8000.438123	12.729408	-0.062482	4.815705
289.936276	8000.434562	12.734413	-0.062457	4.815705
289.976989	8000.440820	12.739418	-0.062466	4.815706
290.253786	8000.496477	12.744423	-0.062519	4.815721
290.300165	8000.478216	12.749427	-0.062529	4.815715
290.305243	8000.440978	12.754432	-0.062532	4.815705
290.015871	8000.458170	12.759437	-0.062479	4.815711
290.123749	8000.459265	12.764442	-0.062501	4.815711
290.199899	8000.393383	12.769447	-0.062516	4.815691
289.864750	8000.412928	12.774451	-0.062455	4.815699
290.004928	8000.414629	12.779456	-0.062483	4.815698
290.039702	8000.418633	12.784461	-0.062490	4.815699
290.093004	8000.435834	12.789466	-0.062502	4.815704
289.898568	8000.439819	12.794471	-0.062467	4.815706
290.194792	8000.439096	12.799475	-0.062524	4.815704
290.298889	8000.457251	12.804480	-0.062544	4.815709
290.026676	8000.452281	12.809485	-0.062495	4.815709
290.172427	8000.441238	12.814490	-0.062524	4.815705
290.215131	8000.417555	12.819495	-0.062533	4.815698
290.194499	8000.428014	12.824499	-0.062530	4.815701
290.062684	8000.444952	12.829504	-0.062507	4.815706
290.129295	8000.424929	12.834509	-0.062521	4.815700
290.113842	8000.445122	12.839514	-0.062520	4.815706
289.881807	8000.458037	12.844519	-0.062478	4.815711
289.916566	8000.451335	12.849523	-0.062486	4.815709
289.978820	8000.448362	12.854528	-0.062499	4.815708
289.811682	8000.430375	12.859533	-0.062469	4.815703
289.821247	8000.436048	12.864538	-0.062472	4.815705
289.920981	8000.450909	12.869543	-0.062492	4.815709
290.045748	8000.424483	12.874547	-0.062517	4.815700
290.127559	8000.470056	12.879552	-0.062533	4.815713
290.207200	8000.432077	12.884557	-0.062549	4.815701
290.287448	8000.445501	12.889562	-0.062566	4.815705
290.192777	8000.434228	12.894567	-0.062550	4.815702
290.184596	8000.442780	12.899571	-0.062549	4.815705
290.347695	8000.504870	12.904576	-0.062581	4.815722
290.237834	8000.439777	12.909581	-0.062562	4.815703
290.177174	8000.456980	12.914586	-0.062552	4.815709
290.241224	8000.502221	12.919591	-0.062566	4.815721
289.918145	8000.464175	12.924595	-0.062507	4.815712
289.993478	8000.489284	12.929600	-0.062522	4.815719
290.093568	8000.439911	12.934605	-0.062542	4.815704
290.172026	8000.492917	12.939610	-0.062558	4.815719
289.926167	8000.435979	12.944615	-0.062514	4.815704
290.063490	8000.430131	12.949619	-0.062541	4.815701
290.038116	8000.447997	12.954624	-0.062537	4.815706
289.967920	8000.427547	12.959629	-0.062526	4.815701
289.996537	8000.461415	12.964634	-0.062533	4.815710
290.063496	8000.469237	12.969639	-0.062546	4.815712
290.112820	8000.455313	12.974643	-0.062557	4.815708
290.112782	8000.472584	12.979648	-0.062558	4.815713
289.898273	8000.425870	12.984653	-0.062520	4.815700
290.066638	8000.450585	12.989658	-0.062553	4.815707
289.964269	8000.438096	12.994663	-0.062535	4.815704
290.146485	8000.435233	12.999667	-0.062570	4.815702
290.258367	8000.452463	13.004672	-0.062592	4.815706
290.206063	8000.417360	13.009677	-0.062584	4.815696
290.123004	8000.426648	13.014682	-0.062570	4.815699
290.028966	8000.421811	13.019687	-0.062554	4.815698
289.836574	8000.433328	13.024691	-0.062519	4.815703
290.002926	8000.449440	13.029696	-0.062552	4.815706
290.065569	8000.432554	13.034701	-0.062565	4.815701
289.992866	8000.462379	13.039706	-0.062553	4.815710
290.122052	8000.460662	13.044711	-0.062578	4.815709
290.006547	8000.443645	13.049715	-0.062558	4.815705
290.303478	8000.450430	13.054720	-0.062615	4.815705
290.315670	8000.431527	13.059725	-0.062618	4.815699
290.093530	8000.454264	13.064730	-0.062578	4.815707
289.998926	8000.521151	13.069735	-0.062562	4.815727
290.097800	8000.482462	13.074739	-0.062582	4.815715
290.148164	8000.455710	13.079744	-0.062593	4.815707
290.078185	8000.418134	13.084749	-0.062581	4.815696
290.130530	8000.447094	13.089754	-0.062592	4.815705
290.089165	8000.467871	13.094759	-0.062586	4.815711
290.038276	8000.455279	13.099763	-0.062578	4.815707
290.242362	8000.461392	13.104768	-0.062617	4.815708
290.122598	8000.418598	13.109773	-0.062596	4.815696
290.115461	8000.473209	13.114778	-0.062596	4.815712
290.045378	8000.435630	13.119783	-0.062585	4.815701
289.934918	8000.429414	13.124787	-0.062566	4.815700
289.955122	8000.449206	13.129792	-0.062571	4.815706
289.963591	8000.446293	13.134797	-0.062574	4.815705
290.240683	8000.469837	13.139802	-0.062627	4.815710
290.003151	8000.414125	13.144807	-0.062584	4.815695
289.911897	8000.429683	13.149811	-0.062568	4.815700
290.027749	8000.450200	13.154816	-0.062591	4.815705
290.127756	8000.439370	13.159821	-0.062611	4.815702
290.021850	8000.449299	13.164826	-0.062593	4.815705
290.046554	8000.441338	13.169831	-0.062599	4.815703
290.083045	8000.433597	13.174835	-0.062607	4.815700
290.027014	8000.453029	13.179840	-0.062598	4.815706
289.814432	8000.439542	13.184845	-0.062560	4.815703
289.973415	8000.442667	13.189850	-0.062591	4.815703
290.159834	8000.474145	13.194855	-0.062627	4.815711
290.079039	8000.465273	13.199859	-0.062613	4.815709
290.179334	8000.484428	13.204864	-0.062633	4.815714
289.994465	8000.442552	13.209869	-0.062600	4.815703
289.872452	8000.481087	13.214874	-0.062579	4.815715
290.034336	8000.433945	13.219879	-0.062610	4.815700
290.008618	8000.430391	13.224883	-0.062607	4.815699
290.160834	8000.473004	13.229888	-0.062637	4.815711
289.990983	8000.481733	13.234893	-0.062607	4.815714
290.177345	8000.491796	13.239898	-0.062643	4.815716
290.098437	8000.467971	13.244903	-0.062629	4.815710
289.966750	8000.463497	13.249907	-0.062606	4.815709
290.228323	8000.444994	13.254912	-0.062656	4.815702
290.183631	8000.420740	13.259917	-0.062649	4.815695
289.972632	8000.471523	13.264922	-0.062612	4.815711
289.963213	8000.429730	13.269927	-0.062611	4.815699
290.033176	8000.439749	13.274931	-0.062626	4.815701
290.229366	8000.433937	13.279936	-0.062663	4.815699
290.133748	8000.431211	13.284941	-0.062647	4.815698
290.137437	8000.468895	13.289946	-0.062649	4.815709
290.263125	8000.448911	13.294951	-0.062674	4.815703
290.183517	8000.422930	13.299955	-0.062661	4.815695
290.079856	8000.457527	13.304960	-0.062643	4.815706
289.908830	8000.435184	13.309965	-0.062612	4.815700
290.136119	8000.451370	13.314970	-0.062656	4.815704
289.841822	8000.460973	13.319975	-0.062602	4.815708
289.826482	8000.434059	13.324979	-0.062601	4.815700
289.928207	8000.448957	13.329984	-0.062621	4.815704
289.850582	8000.417661	13.334989	-0.062608	4.815695
289.992758	8000.469722	13.339994	-0.062636	4.815710
290.001949	8000.462540	13.344999	-0.062639	4.815708
289.756090	8000.443074	13.350003	-0.062595	4.815703
289.955936	8000.478017	13.355008	-0.062633	4.815712
290.082518	8000.471968	13.360013	-0.062658	4.815710
290.053768	8000.473710	13.365018	-0.062654	4.815710
289.858967	8000.447708	13.370023	-0.062620	4.815704
289.940883	8000.448316	13.375027	-0.062636	4.815704
290.051732	8000.498719	13.380032	-0.062658	4.815718
289.953086	8000.462745	13.385037	-0.062641	4.815708
290.070780	8000.488650	13.390042	-0.062665	4.815715
290.335747	8000.510898	13.395047	-0.062715	4.815720
290.020347	8000.471923	13.400051	-0.062658	4.815710
290.231046	8000.474950	13.405056	-0.062699	4.815710
289.992668	8000.421362	13.410061	-0.062656	4.815695
290.093614	8000.456589	13.415066	-0.062676	4.815705
290.172503	8000.468918	13.420071	-0.062692	4.815708
290.184546	8000.455365	13.425075	-0.062695	4.815704
290.118859	8000.493887	13.430080	-0.062685	4.815715
289.985358	8000.454046	13.435085	-0.062661	4.815705
289.959344	8000.452628	13.440090	-0.062658	4.815704
290.019809	8000.504226	13.445095	-0.062670	4.815719
290.092033	8000.467177	13.450099	-0.062685	4.815708
290.155387	8000.494204	13.455104	-0.062698	4.815715
290.113169	8000.459289	13.460109	-0.062692	4.815705
290.052202	8000.496830	13.465114	-0.062682	4.815716
289.965974	8000.483573	13.470119	-0.062667	4.815713
290.012031	8000.444963	13.475123	-0.062677	4.815701
290.093603	8000.476614	13.480128	-0.062694	4.815710
289.952830	8000.440919	13.485133	-0.062669	4.815700
290.006933	8000.468843	13.490138	-0.062681	4.815708
290.064094	8000.446501	13.495143	-0.062693	4.815701
290.055374	8000.429347	13.500147	-0.062692	4.815696
289.909084	8000.487769	13.505152	-0.062666	4.815714
289.913196	8000.464432	13.510157	-0.062669	4.815707
289.999675	8000.464055	13.515162	-0.062686	4.815707
289.981056	8000.445643	13.520167	-0.062684	4.815701
289.935249	8000.455630	13.525171	-0.062677	4.815705
290.144174	8000.501451	13.530176	-0.062717	4.815717
290.180161	8000.458369	13.535181	-0.062725	4.815704
290.085086	8000.450300	13.540186	-0.062709	4.815702
290.208026	8000.451678	13.545191	-0.062733	4.815702
289.965239	8000.437623	13.550195	-0.062689	4.815699
290.197004	8000.484943	13.555200	-0.062734	4.815711
290.229293	8000.442862	13.560205	-0.062741	4.815699
290.178524	8000.485947	13.565210	-0.062733	4.815712
290.159082	8000.455743	13.570215	-0.062731	4.815703
289.869676	8000.452590	13.575219	-0.062679	4.815704
290.213346	8000.481669	13.580224	-0.062744	4.815710
290.017421	8000.454574	13.585229	-0.062709	4.815703
289.913386	8000.446337	13.590234	-0.062691	4.815701
290.139893	8000.446448	13.595239	-0.062734	4.815700
290.129527	8000.458171	13.600243	-0.062734	4.815704
290.003906	8000.449528	13.605248	-0.062712	4.815702
289.832295	8000.466789	13.610253	-0.062681	4.815708
290.036793	8000.452568	13.615258	-0.062721	4.815702
290.241654	8000.439424	13.620263	-0.062760	4.815697
289.984886	8000.460439	13.625267	-0.062714	4.815705
290.063764	8000.490969	13.630272	-0.062730	4.815713
290.298081	8000.437693	13.635277	-0.062775	4.815696
290.245620	8000.387596	13.640282	-0.062767	4.815682
290.202848	8000.451174	13.645287	-0.062760	4.815701
290.244205	8000.453162	13.650291	-0.062769	4.815701
290.264570	8000.486877	13.655296	-0.062774	4.815711
290.137966	8000.452518	13.660301	-0.062752	4.815701
290.236962	8000.483427	13.665306	-0.062772	4.815710
290.267990	8000.502352	13.670311	-0.062779	4.815715
289.941150	8000.468515	13.675315	-0.062720	4.815707
290.068637	8000.488181	13.680320	-0.062745	4.815712
289.907213	8000.454239	13.685325	-0.062716	4.815703
290.027485	8000.476982	13.690330	-0.062740	4.815709
290.149823	8000.440875	13.695335	-0.062764	4.815698
290.172487	8000.439299	13.700339	-0.062770	4.815697
290.127114	8000.504971	13.705344	-0.062763	4.815716
290.168198	8000.457701	13.710349	-0.062772	4.815702
289.991149	8000.449163	13.715354	-0.062740	4.815701
290.134194	8000.470191	13.720359	-0.062768	4.815706
290.121746	8000.462603	13.725363	-0.062767	4.815704
290.308419	8000.481239	13.730368	-0.062803	4.815708
290.135345	8000.474917	13.735373	-0.062773	4.815707
290.174625	8000.471512	13.740378	-0.062781	4.815706
290.072211	8000.524335	13.745383	-0.062764	4.815722
290.012179	8000.489085	13.750387	-0.062754	4.815712
290.078041	8000.480826	13.755392	-0.062767	4.815709
290.085743	8000.442566	13.760397	-0.062770	4.815698
289.991708	8000.481626	13.765402	-0.062754	4.815710
290.050871	8000.471100	13.770407	-0.062767	4.815706
290.115475	8000.455323	13.775411	-0.062780	4.815701
290.331237	8000.493778	13.780416	-0.062822	4.815711
290.289498	8000.464225	13.785421	-0.062815	4.815703
290.094202	8000.467122	13.790426	-0.062780	4.815705
289.979858	8000.462973	13.795431	-0.062760	4.815704
290.096795	8000.457815	13.800435	-0.062783	4.815702
290.284655	8000.474332	13.805440	-0.062820	4.815706
290.249360	8000.467385	13.810445	-0.062815	4.815704
290.194440	8000.468635	13.815450	-0.062806	4.815705
290.140277	8000.478465	13.820455	-0.062797	4.815708
290.120285	8000.448250	13.825459	-0.062795	4.815699
290.182490	8000.466690	13.830464	-0.062808	4.815704
290.061054	8000.445277	13.835469	-0.062787	4.815698
289.974724	8000.475917	13.840474	-0.062772	4.815708
290.141480	8000.458846	13.845479	-0.062804	4.815702
289.920571	8000.444130	13.850483	-0.062765	4.815699
289.953328	8000.478078	13.855488	-0.062772	4.815708
289.989693	8000.439285	13.860493	-0.062780	4.815697
290.137325	8000.481814	13.865498	-0.062809	4.815708
290.184808	8000.514968	13.870503	-0.062819	4.815718
290.187008	8000.491594	13.875507	-0.062821	4.815711
290.246654	8000.470370	13.880512	-0.062834	4.815704
290.061372	8000.448828	13.885517	-0.062801	4.815699
290.226564	8000.489546	13.890522	-0.062833	4.815710
290.359377	8000.477191	13.895527	-0.062859	4.815705
290.212601	8000.442453	13.900531	-0.062833	4.815696
290.138086	8000.458325	13.905536	-0.062820	4.815701
289.857700	8000.423219	13.910541	-0.062770	4.815692
290.059286	8000.462479	13.915546	-0.062808	4.815703
290.177537	8000.493750	13.920551	-0.062832	4.815711
289.819463	8000.453972	13.925555	-0.062767	4.815701
289.854536	8000.484751	13.930560	-0.062775	4.815710
290.032901	8000.436847	13.935565	-0.062809	4.815695
290.272342	8000.446839	13.940570	-0.062855	4.815697
290.033802	8000.476761	13.945575	-0.062812	4.815707
290.099167	8000.446008	13.950579	-0.062826	4.815697
290.071907	8000.486323	13.955584	-0.062822	4.815709
289.859108	8000.459982	13.960589	-0.062784	4.815703
289.896662	8000.492948	13.965594	-0.062792	4.815712
290.081187	8000.504050	13.970599	-0.062828	4.815714
290.140440	8000.482818	13.975603	-0.062840	4.815708
290.250199	8000.477526	13.980608	-0.062862	4.815705
290.176557	8000.438808	13.985613	-0.062850	4.815695
290.214317	8000.487839	13.990618	-0.062858	4.815709
290.026712	8000.464112	13.995623	-0.062825	4.815703
289.904893	8000.461964	14.000627	-0.062803	4.815703
290.270635	8000.502167	14.005632	-0.062873	4.815712
290.196712	8000.491282	14.010637	-0.062861	4.815710
289.980137	8000.465940	14.015642	-0.062822	4.815703
290.293163	8000.462324	14.020647	-0.062881	4.815700
290.149879	8000.455490	14.025651	-0.062856	4.815699
290.058564	8000.488177	14.030656	-0.062840	4.815709
289.971427	8000.472762	14.035661	-0.062826	4.815705
290.050637	8000.497946	14.040666	-0.062842	4.815712
290.194427	8000.470807	14.045671	-0.062870	4.815703
290.101964	8000.449938	14.050675	-0.062854	4.815698
290.221757	8000.482308	14.055680	-0.062878	4.815706
290.147553	8000.439297	14.060685	-0.062865	4.815694
289.927909	8000.452443	14.065690	-0.062826	4.815699
290.159292	8000.436586	14.070695	-0.062870	4.815693
289.953132	8000.444631	14.075699	-0.062833	4.815697
290.159272	8000.492543	14.080704	-0.062873	4.815710
290.022522	8000.475125	14.085709	-0.062849	4.815705
290.336990	8000.501517	14.090714	-0.062909	4.815711
289.919703	8000.575192	14.095719	-0.062833	4.815735
289.870618	8000.526228	14.100723	-0.062825	4.815721
290.150439	8000.548757	14.105728	-0.062878	4.815726
289.945233	8000.471162	14.110733	-0.062842	4.815704
290.135372	8000.502713	14.115738	-0.062878	4.815712
290.155771	8000.466832	14.120743	-0.062883	4.815702
290.145296	8000.472130	14.125747	-0.062883	4.815703
290.137736	8000.482835	14.130752	-0.062883	4.815706
290.316382	8000.452069	14.135757	-0.062918	4.815696
290.236722	8000.396106	14.140762	-0.062904	4.815680
290.323106	8000.497446	14.145767	-0.062922	4.815710
290.264882	8000.454734	14.150771	-0.062912	4.815697
290.356356	8000.486573	14.155776	-0.062931	4.815706
290.136795	8000.483659	14.160781	-0.062891	4.815706
290.221264	8000.473609	14.165786	-0.062908	4.815703
290.303233	8000.489208	14.170791	-0.062925	4.815707
290.154290	8000.467278	14.175795	-0.062899	4.815701
290.118800	8000.501014	14.180800	-0.062893	4.815711
290.163031	8000.505198	14.185805	-0.062903	4.815712
290.303946	8000.498349	14.190810	-0.062931	4.815710
290.094770	8000.507408	14.195815	-0.062893	4.815713
290.055270	7999.433979	14.200819	-0.062886	4.815400

290.206710	7996.187844	14.205824	-0.062914	4.814453
290.175493	7990.607056	14.210829	-0.062906	4.812825
290.032725	7983.910441	14.215834	-0.062876	4.810872
289.965484	7976.653440	14.220839	-0.062860	4.808753
289.948659	7969.011575	14.225843	-0.062854	4.806521
289.829276	7961.210149	14.230848	-0.062828	4.804242
289.830265	7953.388974	14.235853	-0.062824	4.801956
289.835929	7945.369924	14.240858	-0.062821	4.799610
289.755980	7937.454648	14.245863	-0.062803	4.797294
289.599326	7929.373482	14.250867	-0.062770	4.794929
289.922387	7921.428059	14.255872	-0.062826	4.792600
289.725677	7913.369088	14.260877	-0.062786	4.790239
289.689593	7905.368976	14.265882	-0.062775	4.787894
289.726262	7897.368669	14.270887	-0.062778	4.785547
289.541970	7889.384679	14.275891	-0.062740	4.783204
289.442407	7881.421965	14.280896	-0.062718	4.780866
289.407985	7873.411092	14.285901	-0.062707	4.778513
289.419179	7865.398518	14.290906	-0.062706	4.776158
289.426951	7857.398338	14.295911	-0.062703	4.773805
289.204710	7849.343469	14.300915	-0.062658	4.771436
289.348958	7841.325719	14.305920	-0.062681	4.769075
289.089626	7833.351528	14.310925	-0.062629	4.766728
289.092493	7825.285604	14.315930	-0.062626	4.764351
289.094377	7817.433323	14.320935	-0.062622	4.762036
288.999795	7809.334826	14.325939	-0.062601	4.759648
289.176170	7801.419781	14.330944	-0.062630	4.757311
289.087488	7793.319922	14.335949	-0.062609	4.754920
288.840266	7785.313960	14.340954	-0.062560	4.752556
289.021216	7777.296669	14.345959	-0.062589	4.750186
288.821329	7769.292035	14.350963	-0.062548	4.747820
288.964327	7761.309627	14.355968	-0.062571	4.745458
288.920186	7753.350903	14.360973	-0.062559	4.743102
288.731913	7745.306867	14.365978	-0.062520	4.740721
288.837828	7737.372771	14.370983	-0.062536	4.738369
288.784395	7729.314289	14.375987	-0.062522	4.735981
288.789073	7721.344786	14.380992	-0.062519	4.733617
288.544625	7713.272201	14.385997	-0.062470	4.731222
288.536094	7705.311666	14.391002	-0.062465	4.728859
288.632610	7697.331096	14.396007	-0.062479	4.726488
288.404820	7689.252148	14.401011	-0.062433	4.724088
288.343440	7681.353482	14.406016	-0.062417	4.721740
288.483085	7673.310909	14.411021	-0.062439	4.719347
288.253903	7665.330330	14.416026	-0.062393	4.716972
288.342666	7657.319438	14.421031	-0.062406	4.714586
288.270652	7649.262742	14.426035	-0.062388	4.712186
288.128469	7641.291154	14.431040	-0.062358	4.709810
288.141441	7633.287496	14.436045	-0.062357	4.707423
288.229419	7625.231089	14.441050	-0.062369	4.705019
288.281088	7617.354070	14.446055	-0.062375	4.702667
288.097184	7609.266679	14.451059	-0.062337	4.700252
288.097384	7601.356468	14.456064	-0.062333	4.697888
287.889293	7593.323138	14.461069	-0.062291	4.695486
287.825561	7585.287947	14.466074	-0.062275	4.693083
287.975875	7577.303552	14.471079	-0.062299	4.690693
287.911712	7569.294305	14.476083	-0.062283	4.688294
287.775026	7561.241726	14.481088	-0.062254	4.685882
287.614966	7553.280630	14.486093	-0.062220	4.683496
287.479330	7545.280137	14.491098	-0.062191	4.681097
287.564936	7537.324981	14.496103	-0.062204	4.678709
287.435495	7529.261058	14.501107	-0.062176	4.676288
287.497580	7521.259870	14.506112	-0.062183	4.673885
287.554182	7513.155775	14.511117	-0.062190	4.671449
287.327591	7505.160910	14.516122	-0.062144	4.669045
287.372745	7497.229076	14.521127	-0.062149	4.666659
287.167472	7489.199133	14.526131	-0.062107	4.664242
287.515820	7481.236920	14.531136	-0.062168	4.661843
287.242840	7473.209754	14.536141	-0.062113	4.659425
287.327842	7465.247920	14.541146	-0.062125	4.657025
287.165747	7457.231891	14.546151	-0.062091	4.654607
286.910899	7449.211330	14.551155	-0.062040	4.652187
286.953927	7441.145922	14.556160	-0.062044	4.649751
287.117233	7433.207229	14.561165	-0.062070	4.647353
286.945582	7425.159475	14.566170	-0.062035	4.644920
287.034973	7417.260645	14.571175	-0.062047	4.642531
286.757821	7409.228103	14.576179	-0.061992	4.640101
286.796221	7401.249645	14.581184	-0.061995	4.637686
286.641978	7393.198323	14.586189	-0.061963	4.635247
286.418812	7385.175763	14.591194	-0.061917	4.632816
286.605311	7377.159990	14.596199	-0.061948	4.630385
286.581668	7369.198066	14.601203	-0.061940	4.627970
286.504119	7361.166109	14.606208	-0.061922	4.625532
286.610044	7353.206795	14.611213	-0.061938	4.623114
286.532228	7345.153518	14.616218	-0.061919	4.620667
286.435741	7337.210238	14.621223	-0.061898	4.618253
286.144996	7329.176295	14.626227	-0.061840	4.615809
286.280085	7321.185598	14.631232	-0.061861	4.613377
286.251566	7313.119819	14.636237	-0.061852	4.610921
286.338171	7305.119003	14.641242	-0.061864	4.608483
286.325685	7297.180596	14.646247	-0.061858	4.606063
286.056215	7289.153910	14.651251	-0.061804	4.603615
286.033868	7281.203498	14.656256	-0.061796	4.601189
285.982657	7273.183660	14.661261	-0.061783	4.598741
286.097503	7265.145777	14.666266	-0.061800	4.596285
285.920078	7257.138521	14.671271	-0.061763	4.593838
285.944602	7249.082619	14.676275	-0.061764	4.591374
286.002575	7241.148353	14.681280	-0.061771	4.588947
285.805753	7233.076546	14.686285	-0.061731	4.586476
285.548017	7225.125346	14.691290	-0.061679	4.584040
285.686827	7217.119265	14.696295	-0.061701	4.581586
285.637721	7209.097171	14.701299	-0.061688	4.579127
285.723132	7201.145438	14.706304	-0.061700	4.576687
285.537503	7193.116830	14.711309	-0.061662	4.574223
285.361685	7185.084487	14.716314	-0.061625	4.571756
285.333306	7177.090890	14.721319	-0.061616	4.569299
285.277157	7169.044802	14.726323	-0.061602	4.566825
285.457555	7161.103138	14.731328	-0.061631	4.564382
285.376422	7153.151967	14.736333	-0.061612	4.561935
285.312820	7145.072294	14.741338	-0.061597	4.559447
285.289812	7137.183351	14.746343	-0.061589	4.557016
285.042993	7129.084564	14.751347	-0.061539	4.554519
285.065963	7121.105952	14.756352	-0.061539	4.552058
284.989932	7113.074296	14.761357	-0.061521	4.549579
285.089600	7105.083905	14.766362	-0.061536	4.547112
285.044326	7097.066979	14.771367	-0.061524	4.544635
284.838208	7089.076212	14.776371	-0.061482	4.542164
285.160371	7081.087930	14.781376	-0.061538	4.539694
284.840712	7073.126538	14.786381	-0.061474	4.537230
284.696098	7065.055995	14.791386	-0.061444	4.534731
285.035980	7057.140015	14.796391	-0.061503	4.532278
284.938184	7049.046893	14.801395	-0.061481	4.529770
284.796631	7041.112470	14.806400	-0.061451	4.527309
284.761615	7033.039086	14.811405	-0.061441	4.524803
284.778917	7025.115684	14.816410	-0.061440	4.522343
284.656501	7017.102887	14.821415	-0.061413	4.519854
284.257704	7009.139240	14.826419	-0.061335	4.517377
284.402069	7001.080717	14.831424	-0.061358	4.514871
284.475265	6993.041074	14.836429	-0.061368	4.512370
284.294774	6985.011407	14.841434	-0.061331	4.509869
284.207879	6977.044797	14.846439	-0.061311	4.507387
284.181757	6969.005123	14.851443	-0.061302	4.504881
284.153955	6961.094044	14.856448	-0.061293	4.502414
284.365771	6953.045655	14.861453	-0.061329	4.499903
284.101485	6945.086990	14.866458	-0.061276	4.497418
284.217057	6937.051168	14.871463	-0.061293	4.494907
283.756629	6929.046026	14.876467	-0.061204	4.492404
283.948987	6921.025604	14.881472	-0.061236	4.489896
283.784174	6913.060252	14.886477	-0.061201	4.487403
283.660848	6904.985424	14.891482	-0.061174	4.484875
283.588818	6897.098102	14.896487	-0.061157	4.482404
283.600844	6888.960546	14.901491	-0.061156	4.479853
283.849575	6881.061450	14.906496	-0.061198	4.477377
283.477336	6873.039793	14.911501	-0.061125	4.474858
283.573979	6865.030530	14.916506	-0.061139	4.472344
283.561941	6857.008850	14.921511	-0.061133	4.469824
283.387733	6849.018046	14.926515	-0.061097	4.467311
283.478971	6841.003474	14.931520	-0.061110	4.464791
283.383214	6833.053736	14.936525	-0.061088	4.462289
283.302529	6824.974532	14.941530	-0.061069	4.459745
283.406295	6817.055623	14.946535	-0.061085	4.457251
283.232193	6808.989524	14.951539	-0.061049	4.454707
283.289042	6801.009786	14.956544	-0.061055	4.452191
283.104439	6792.994606	14.961549	-0.061017	4.449661
283.119056	6784.984852	14.966554	-0.061016	4.447131
283.128752	6776.996503	14.971559	-0.061014	4.444608
283.029068	6769.015905	14.976563	-0.060992	4.442084
282.871576	6760.987268	14.981568	-0.060959	4.439544
283.031794	6753.070026	14.986573	-0.060985	4.437039
282.916309	6745.000809	14.991578	-0.060959	4.434484
282.861907	6736.957228	14.996583	-0.060945	4.431935
282.934288	6728.933478	15.001587	-0.060955	4.429391
282.719257	6720.959226	15.006592	-0.060911	4.426861
282.675446	6712.988436	15.011597	-0.060899	4.424331
282.747686	6704.967664	15.016602	-0.060909	4.421784
282.802319	6696.991991	15.021607	-0.060915	4.419250
282.622528	6688.934657	15.026611	-0.060878	4.416687
282.491018	6680.945196	15.031616	-0.060850	4.414145
282.523364	6672.960118	15.036621	-0.060852	4.411603
282.466041	6664.920121	15.041626	-0.060837	4.409042
282.492807	6656.942403	15.046631	-0.060838	4.406500
282.544099	6648.948380	15.051635	-0.060844	4.403951
282.603135	6640.972552	15.056640	-0.060851	4.401407
282.461736	6632.941682	15.061645	-0.060821	4.398843
282.408671	6624.987529	15.066650	-0.060807	4.396302
282.285998	6616.973619	15.071655	-0.060781	4.393740
282.137342	6608.927748	15.076659	-0.060749	4.391166
281.978850	6600.967767	15.081664	-0.060716	4.388618
281.882945	6592.940338	15.086669	-0.060694	4.386047
282.113210	6584.928090	15.091674	-0.060733	4.383482
282.087270	6576.971283	15.096679	-0.060725	4.380931
282.063485	6568.967516	15.101683	-0.060716	4.378364
282.039385	6560.956793	15.106688	-0.060708	4.375793
281.892320	6552.987824	15.111693	-0.060677	4.373233
281.782940	6544.948156	15.116698	-0.060653	4.370649
281.777097	6536.975605	15.121703	-0.060648	4.368086
281.717618	6528.915522	15.126707	-0.060633	4.365493
281.682287	6521.007223	15.131712	-0.060623	4.362947
281.657307	6512.970614	15.136717	-0.060614	4.360359
281.566913	6504.993222	15.141722	-0.060593	4.357788
281.387611	6496.975716	15.146727	-0.060556	4.355201
281.350552	6488.834714	15.151731	-0.060545	4.352574
281.387149	6480.862609	15.156736	-0.060548	4.350001
281.289855	6472.917985	15.161741	-0.060526	4.347434
281.156552	6464.887041	15.166746	-0.060498	4.344837
281.370426	6456.969218	15.171751	-0.060534	4.342278
281.088708	6448.915976	15.176755	-0.060478	4.339670
281.099894	6440.988297	15.181760	-0.060476	4.337103
281.188674	6432.950129	15.186765	-0.060489	4.334500
281.210765	6424.863200	15.191770	-0.060489	4.331878
281.099511	6416.917555	15.196775	-0.060464	4.329300
281.145337	6408.920648	15.201779	-0.060469	4.326705
281.132637	6400.916261	15.206784	-0.060463	4.324105
280.726511	6392.995834	15.211789	-0.060383	4.321528
280.617857	6384.928249	15.216794	-0.060359	4.318904
280.932467	6376.942143	15.221799	-0.060414	4.316308
280.527489	6368.955766	15.226803	-0.060335	4.313705
280.393994	6360.912072	15.231808	-0.060306	4.311084
280.584425	6352.925735	15.236813	-0.060338	4.308482
280.576520	6344.898690	15.241818	-0.060332	4.305864
280.468317	6336.941848	15.246823	-0.060309	4.303266
280.244673	6328.928371	15.251827	-0.060263	4.300648
280.286986	6320.955020	15.256832	-0.060267	4.298043
280.479353	6312.894345	15.261837	-0.060299	4.295409
280.326425	6304.849227	15.266842	-0.060267	4.292776
280.425009	6296.906332	15.271847	-0.060281	4.290177
280.077728	6288.917511	15.276851	-0.060213	4.287557
280.277665	6280.864817	15.281856	-0.060246	4.284919
280.041928	6272.915720	15.286861	-0.060199	4.282311
279.870611	6264.899666	15.291866	-0.060163	4.279679
280.122370	6256.936515	15.296871	-0.060206	4.277066
280.221161	6248.882069	15.301875	-0.060220	4.274420
280.120941	6240.867773	15.306880	-0.060198	4.271785
279.957359	6232.864758	15.311885	-0.060164	4.269151
279.678541	6224.851576	15.316890	-0.060108	4.266511
279.861658	6216.888865	15.321895	-0.060138	4.263890
279.684686	6208.871804	15.326899	-0.060101	4.261246
279.608007	6200.897961	15.331904	-0.060083	4.258616
279.392478	6192.893829	15.336909	-0.060039	4.255972
279.519569	6184.852914	15.341914	-0.060059	4.253318
279.659415	6176.820420	15.346919	-0.060081	4.250666
279.523780	6168.886894	15.351923	-0.060052	4.248042
279.614217	6160.839203	15.356928	-0.060065	4.245380
279.729501	6152.923153	15.361933	-0.060083	4.242761
279.355632	6144.880779	15.366938	-0.060010	4.240094
279.460935	6136.956982	15.371943	-0.060025	4.237468
279.542365	6128.855194	15.376947	-0.060037	4.234782
279.417356	6120.887323	15.381952	-0.060010	4.232137
279.200725	6112.846167	15.386957	-0.059965	4.229465
279.123137	6104.870227	15.391962	-0.059947	4.226814
279.151193	6096.868236	15.396967	-0.059949	4.224154
279.126691	6088.934661	15.401971	-0.059940	4.221514
279.083999	6080.891262	15.406976	-0.059928	4.218836
279.120727	6072.911642	15.411981	-0.059931	4.216178
278.925107	6064.870638	15.416986	-0.059891	4.213496
279.030560	6056.881401	15.421991	-0.059907	4.210832
279.110932	6048.887619	15.426995	-0.059918	4.208165
278.964601	6040.911082	15.432000	-0.059887	4.205500
278.915841	6032.932138	15.437005	-0.059874	4.202833
278.905143	6024.887161	15.442010	-0.059868	4.200143
279.094195	6016.980394	15.447015	-0.059900	4.197499
278.657949	6008.930368	15.452019	-0.059815	4.194800
278.563164	6000.792532	15.457024	-0.059793	4.192072
278.572644	5992.805827	15.462029	-0.059791	4.189395
278.313028	5984.845453	15.467034	-0.059739	4.186722
278.544078	5976.848263	15.472039	-0.059778	4.184040
278.359717	5968.883799	15.477043	-0.059740	4.181363
278.395015	5960.886123	15.482048	-0.059743	4.178675
278.369039	5952.887147	15.487053	-0.059734	4.175984
278.052689	5944.885781	15.492058	-0.059671	4.173288
278.078614	5936.886303	15.497063	-0.059672	4.170594
278.119766	5928.855384	15.502067	-0.059676	4.167889
278.088248	5920.882899	15.507072	-0.059667	4.165200
277.908139	5912.938868	15.512077	-0.059629	4.162518
277.913960	5904.867374	15.517082	-0.059626	4.159792
277.853224	5896.941902	15.522087	-0.059611	4.157114
277.795488	5888.862691	15.527091	-0.059597	4.154382
277.819417	5880.857160	15.532096	-0.059597	4.151674
277.712645	5872.858423	15.537101	-0.059574	4.148965
277.762465	5864.828402	15.542106	-0.059579	4.146245
277.784386	5856.887435	15.547111	-0.059579	4.143554
277.736422	5848.883137	15.552115	-0.059567	4.140838
277.642799	5840.907734	15.557120	-0.059545	4.138130
277.742936	5832.873081	15.562125	-0.059560	4.135403
277.428222	5824.853364	15.567130	-0.059498	4.132673
277.256061	5816.869023	15.572135	-0.059462	4.129956
277.231606	5808.854612	15.577139	-0.059453	4.127228
277.458763	5800.839465	15.582144	-0.059492	4.124502
277.369672	5792.886443	15.587149	-0.059472	4.121790
277.348278	5784.865827	15.592154	-0.059464	4.119055
277.387904	5776.904175	15.597159	-0.059467	4.116339
277.191131	5768.855674	15.602163	-0.059427	4.113589
277.264022	5760.835832	15.607168	-0.059437	4.110849
277.256696	5752.875326	15.612173	-0.059431	4.108128
277.171655	5744.797956	15.617178	-0.059412	4.105363
277.159180	5736.886589	15.622183	-0.059406	4.102654
277.198775	5728.851007	15.627187	-0.059409	4.099902
276.969501	5720.904476	15.632192	-0.059363	4.097175
276.908410	5712.870666	15.637197	-0.059347	4.094418
276.810682	5704.825481	15.642202	-0.059325	4.091655
276.884124	5696.850219	15.647207	-0.059335	4.088917
276.946991	5688.842541	15.652211	-0.059343	4.086165
276.838105	5680.893924	15.657216	-0.059319	4.083429
276.932590	5672.872214	15.662221	-0.059333	4.080670
276.730252	5664.924344	15.667226	-0.059291	4.077929
276.631622	5656.927207	15.672231	-0.059269	4.075172
276.574868	5648.896811	15.677235	-0.059255	4.072401
276.568856	5640.875361	15.682240	-0.059250	4.069633
276.415326	5632.934717	15.687245	-0.059217	4.066888
276.327695	5624.871399	15.692250	-0.059197	4.064100
276.313637	5616.918133	15.697255	-0.059191	4.061349
276.356887	5608.901263	15.702259	-0.059195	4.058575
276.495982	5600.888743	15.707264	-0.059217	4.055802
276.547497	5592.905869	15.712269	-0.059223	4.053037
276.424038	5584.861676	15.717274	-0.059196	4.050245
276.024121	5576.963762	15.722279	-0.059118	4.047499
276.114836	5568.881595	15.727283	-0.059131	4.044693
276.022102	5560.936421	15.732288	-0.059110	4.041931
275.882329	5552.979806	15.737293	-0.059080	4.039162
275.763496	5544.939062	15.742298	-0.059054	4.036362
276.003603	5536.831729	15.747303	-0.059095	4.033543
275.818560	5528.785275	15.752307	-0.059057	4.030736
275.442440	5520.914479	15.757312	-0.058983	4.027986
275.611175	5512.861779	15.762317	-0.059010	4.025178
275.430144	5504.911610	15.767322	-0.058973	4.022399
275.586819	5496.883932	15.772327	-0.058998	4.019596
275.303604	5488.936751	15.777331	-0.058942	4.016813
275.241073	5480.887659	15.782336	-0.058926	4.013995
275.057391	5472.894016	15.787341	-0.058888	4.011193
275.025204	5464.843394	15.792346	-0.058878	4.008372
275.058469	5456.902411	15.797351	-0.058881	4.005588
275.083658	5448.858795	15.802355	-0.058882	4.002765
274.952356	5440.862354	15.807360	-0.058853	3.999955
275.111214	5432.921888	15.812365	-0.058879	3.997167
275.304101	5424.832757	15.817370	-0.058911	3.994326
274.993595	5416.868294	15.822375	-0.058849	3.991518
274.746632	5408.885470	15.827379	-0.058800	3.988703
274.910991	5400.818257	15.832384	-0.058826	3.985862
274.829740	5392.930592	15.837389	-0.058808	3.983079
274.742051	5384.846264	15.842394	-0.058787	3.980225
274.994489	5376.936162	15.847399	-0.058831	3.977436
274.897743	5368.894635	15.852403	-0.058809	3.974592
274.668343	5360.924094	15.857408	-0.058762	3.971769
274.533327	5352.910898	15.862413	-0.058733	3.968931
274.424069	5344.881161	15.867418	-0.058709	3.966085
274.655741	5336.923337	15.872423	-0.058748	3.963269
274.844450	5328.867489	15.877427	-0.058780	3.960415
274.711714	5320.914152	15.882432	-0.058751	3.957590
274.692279	5312.910281	15.887437	-0.058744	3.954746
274.357224	5304.878751	15.892442	-0.058677	3.951886
274.396041	5296.931136	15.897447	-0.058681	3.949060
274.305792	5288.912037	15.902451	-0.058660	3.946204
274.194210	5280.925210	15.907456	-0.058636	3.943357
274.205324	5272.958463	15.912461	-0.058634	3.940517
274.410002	5264.905925	15.917466	-0.058668	3.937648
274.119079	5256.967882	15.922471	-0.058610	3.934809
273.880358	5248.943193	15.927475	-0.058562	3.931938
273.709628	5240.984011	15.932480	-0.058526	3.929089
274.097651	5232.958902	15.937485	-0.058595	3.926225
273.712230	5224.953882	15.942490	-0.058519	3.923352
273.935443	5216.927542	15.947495	-0.058557	3.920480
273.960949	5208.965503	15.952499	-0.058558	3.917626
274.137442	5200.941758	15.957504	-0.058587	3.914750
273.792512	5192.969803	15.962509	-0.058519	3.911881
273.745847	5184.923798	15.967514	-0.058506	3.908989
273.730809	5176.958549	15.972519	-0.058500	3.906124
273.413819	5168.960610	15.977523	-0.058437	3.903240
273.714281	5160.929680	15.982528	-0.058489	3.900353
273.423743	5153.023775	15.987533	-0.058431	3.897498
273.482594	5144.928606	15.992538	-0.058438	3.894579
273.524834	5136.968289	15.997543	-0.058442	3.891707
273.525901	5128.930423	16.002547	-0.058439	3.888803
273.459571	5120.956426	16.007552	-0.058422	3.885920
273.434161	5112.982810	16.012557	-0.058414	3.883035
273.218655	5104.964676	16.017562	-0.058370	3.880128
273.306120	5097.010056	16.022567	-0.058382	3.877247
273.285025	5088.949082	16.027571	-0.058375	3.874324
273.192835	5080.736256	16.032576	-0.058354	3.871342
273.112856	5072.836812	16.037581	-0.058335	3.868472
273.357202	5064.835929	16.042586	-0.058377	3.865569
273.297611	5056.927470	16.047591	-0.058362	3.862692
273.161083	5048.904706	16.052595	-0.058332	3.859770
273.096648	5040.973328	16.057600	-0.058317	3.856880
272.980013	5032.977957	16.062605	-0.058291	3.853963
272.799461	5024.913434	16.067610	-0.058254	3.851018
272.788011	5016.970818	16.072615	-0.058248	3.848118
272.389787	5009.008223	16.077619	-0.058170	3.845201
272.568672	5000.959786	16.082624	-0.058199	3.842262
272.646780	4992.969003	16.087629	-0.058210	3.839340
272.199655	4985.010552	16.092634	-0.058123	3.836417
272.355595	4977.013215	16.097639	-0.058148	3.833489
272.500314	4968.943407	16.102643	-0.058171	3.830533
272.426013	4960.948892	16.107648	-0.058154	3.827597
272.551841	4952.946853	16.112653	-0.058173	3.824661
272.691862	4944.976434	16.117658	-0.058195	3.821734
272.578122	4937.007629	16.122663	-0.058170	3.818800
272.296516	4929.027320	16.127667	-0.058114	3.815856
272.423881	4921.027663	16.132672	-0.058134	3.812912
272.379219	4913.000717	16.137677	-0.058122	3.809951
272.296006	4905.015207	16.142682	-0.058103	3.807003
272.200343	4897.045928	16.147687	-0.058081	3.804058
272.192874	4889.088794	16.152691	-0.058076	3.801117
272.234541	4881.090285	16.157696	-0.058080	3.798159
272.200727	4873.062718	16.162701	-0.058070	3.795187
271.972830	4864.999610	16.167706	-0.058023	3.792195
272.103235	4857.014769	16.172711	-0.058044	3.789238
271.844734	4849.027629	16.177715	-0.057992	3.786269
271.823463	4841.061588	16.182720	-0.057984	3.783310
271.626165	4833.065920	16.187725	-0.057944	3.780335
271.584841	4825.073339	16.192730	-0.057932	3.777361
271.547869	4817.049926	16.197735	-0.057921	3.774374
271.441996	4809.056230	16.202739	-0.057898	3.771394
271.483803	4801.040042	16.207744	-0.057902	3.768407
271.613813	4793.033303	16.212749	-0.057922	3.765422
271.428921	4785.070907	16.217754	-0.057884	3.762445
271.286461	4777.088969	16.222759	-0.057854	3.759459
271.128110	4769.126076	16.227763	-0.057820	3.756478
271.315086	4761.041177	16.232768	-0.057851	3.753456
271.177098	4753.069031	16.237773	-0.057822	3.750467
271.159214	4745.056051	16.242778	-0.057815	3.747463
271.215797	4737.039979	16.247783	-0.057821	3.744456
270.982169	4729.117049	16.252787	-0.057774	3.741476
271.036566	4721.066609	16.257792	-0.057780	3.738452
271.130067	4713.086636	16.262797	-0.057794	3.735453
270.888261	4705.045023	16.267802	-0.057745	3.732421
270.997643	4697.056234	16.272807	-0.057762	3.729414
270.908309	4689.075428	16.277811	-0.057741	3.726403
270.975421	4681.082266	16.282816	-0.057750	3.723389
271.030761	4673.114468	16.287821	-0.057756	3.720381
270.578103	4665.172562	16.292826	-0.057668	3.717369
270.503956	4657.163982	16.297831	-0.057651	3.714338
270.388743	4649.039264	16.302835	-0.057625	3.711260
270.338263	4641.065505	16.307840	-0.057612	3.708238
270.341527	4633.095682	16.312845	-0.057609	3.705216
270.326410	4625.115442	16.317850	-0.057602	3.702188
270.369582	4617.165955	16.322855	-0.057606	3.699170
270.271813	4609.147409	16.327859	-0.057584	3.696119
270.226933	4601.137871	16.332864	-0.057572	3.693071
270.300067	4593.101132	16.337869	-0.057582	3.690013
270.296731	4585.130840	16.342874	-0.057578	3.686976
270.174296	4577.168298	16.347879	-0.057551	3.683937
270.005016	4569.191722	16.352883	-0.057516	3.680888
269.947564	4561.218621	16.357888	-0.057501	3.677841
270.133612	4553.197041	16.362893	-0.057532	3.674779
270.007054	4545.162624	16.367898	-0.057504	3.671702
270.075471	4537.171058	16.372903	-0.057513	3.668643
269.867314	4529.179152	16.377907	-0.057471	3.665575
269.872972	4521.183941	16.382912	-0.057468	3.662508
269.633534	4513.192198	16.387917	-0.057420	3.659434
269.478521	4505.256069	16.392922	-0.057387	3.656380
269.603576	4497.220293	16.397927	-0.057406	3.653293
269.513036	4489.179759	16.402931	-0.057386	3.650196
269.531711	4481.215708	16.407936	-0.057385	3.647129
269.660282	4473.193480	16.412941	-0.057406	3.644039
269.491291	4465.216712	16.417946	-0.057370	3.640957
269.636350	4457.236802	16.422951	-0.057393	3.637879
269.404846	4449.260926	16.427955	-0.057347	3.634790
269.176980	4441.233611	16.432960	-0.057300	3.631679
269.194301	4433.222306	16.437965	-0.057300	3.628577
269.298991	4425.196555	16.442970	-0.057315	3.625470
269.159684	4417.264415	16.447975	-0.057286	3.622390
268.983528	4409.268475	16.452979	-0.057249	3.619281
269.072584	4401.241067	16.457984	-0.057262	3.616165
269.252285	4393.221478	16.462989	-0.057291	3.613051
268.888284	4385.219274	16.467994	-0.057220	3.609927
268.848931	4377.284837	16.472999	-0.057209	3.606835
268.859660	4369.270479	16.478003	-0.057207	3.603711
268.861139	4361.309301	16.483008	-0.057203	3.600605
268.864268	4353.333305	16.488013	-0.057200	3.597490
268.784447	4345.299017	16.493018	-0.057181	3.594347
268.762011	4337.306820	16.498023	-0.057173	3.591220
268.778902	4329.306058	16.503027	-0.057173	3.588088
268.813219	4321.281578	16.508032	-0.057175	3.584944
268.717522	4313.367266	16.513037	-0.057154	3.581837
268.604737	4305.349812	16.518042	-0.057129	3.578686
268.664566	4297.364421	16.523047	-0.057136	3.575550
268.710332	4289.332275	16.528051	-0.057141	3.572392
268.249591	4281.364333	16.533056	-0.057051	3.569243
268.225115	4273.393489	16.538061	-0.057043	3.566102
267.974418	4265.422335	16.543066	-0.056992	3.562952
268.111804	4257.389036	16.548071	-0.057014	3.559785
268.225851	4249.407180	16.553075	-0.057032	3.556635
267.990277	4241.329246	16.558080	-0.056984	3.553434
268.023243	4233.279242	16.563085	-0.056986	3.550250
267.955594	4225.292682	16.568090	-0.056970	3.547084
267.981640	4217.341016	16.573095	-0.056971	3.543933
267.924649	4209.356149	16.578099	-0.056956	3.540763
267.801951	4201.386468	16.583104	-0.056930	3.537594
267.772290	4193.384896	16.588109	-0.056920	3.534412
268.035936	4185.341267	16.593114	-0.056966	3.531219
267.956731	4177.393061	16.598119	-0.056947	3.528052
267.803317	4169.419223	16.603123	-0.056915	3.524869
267.652188	4161.443886	16.608128	-0.056883	3.521683
267.657697	4153.424205	16.613133	-0.056880	3.518480
267.607112	4145.442598	16.618138	-0.056867	3.515289
267.827038	4137.427537	16.623143	-0.056904	3.512089
267.584856	4129.411063	16.628147	-0.056855	3.508872
267.470093	4121.412616	16.633152	-0.056830	3.505663
267.304457	4113.487652	16.638157	-0.056795	3.502479
267.206549	4105.463771	16.643162	-0.056773	3.499254
267.402537	4097.491603	16.648167	-0.056806	3.496056
267.355172	4089.473180	16.653171	-0.056793	3.492829
267.269170	4081.453540	16.658176	-0.056773	3.489598
267.204790	4073.528743	16.663181	-0.056757	3.486402
267.133992	4065.506536	16.668186	-0.056740	3.483164
267.097376	4057.530906	16.673191	-0.056730	3.479942
267.026412	4049.586198	16.678195	-0.056713	3.476730
266.972709	4041.522555	16.683200	-0.056699	3.473466
266.988653	4033.522729	16.688205	-0.056698	3.470228
266.774969	4025.522944	16.693210	-0.056654	3.466979
266.969696	4017.551765	16.698215	-0.056687	3.463752
266.849594	4009.558913	16.703219	-0.056661	3.460503
266.693485	4001.561878	16.708224	-0.056628	3.457248
266.837922	3993.572453	16.713229	-0.056651	3.454002
266.522298	3985.573312	16.718234	-0.056588	3.450735
266.531578	3977.598939	16.723239	-0.056586	3.447486
266.581768	3969.575281	16.728243	-0.056592	3.444214
266.225384	3961.649781	16.733248	-0.056522	3.440966
266.210442	3953.649621	16.738253	-0.056515	3.437696
266.426112	3945.570688	16.743258	-0.056551	3.434398
266.676889	3937.573550	16.748263	-0.056594	3.431131
266.243601	3929.598749	16.753267	-0.056510	3.427848
265.978741	3921.647072	16.758272	-0.056457	3.424577
266.151475	3913.641814	16.763277	-0.056485	3.421295
266.069036	3905.651989	16.768282	-0.056466	3.418008
265.897642	3897.665760	16.773287	-0.056430	3.414716
265.850936	3889.661224	16.778291	-0.056417	3.411418
266.011315	3881.608150	16.783296	-0.056443	3.408103
265.856070	3873.671145	16.788301	-0.056411	3.404822
265.786358	3865.705370	16.793306	-0.056394	3.401530
265.631688	3857.730951	16.798311	-0.056361	3.398227
265.910978	3849.701363	16.803315	-0.056410	3.394913
265.680024	3841.620816	16.808320	-0.056363	3.391558
265.640468	3833.669430	16.813325	-0.056352	3.388259
265.335674	3825.667446	16.818330	-0.056291	3.384927
265.469992	3817.754763	16.823335	-0.056312	3.381644
265.579978	3809.750457	16.828339	-0.056329	3.378319
265.570314	3801.716789	16.833344	-0.056323	3.374974
265.298395	3793.790985	16.838349	-0.056269	3.371661
265.200088	3785.753766	16.843354	-0.056247	3.368305
265.300624	3777.762376	16.848359	-0.056262	3.364972
265.406248	3769.814261	16.853363	-0.056277	3.361654
265.158674	3761.826324	16.858368	-0.056228	3.358303
265.359787	3753.826983	16.863373	-0.056261	3.354960
265.177758	3745.802651	16.868378	-0.056223	3.351589
265.151859	3737.834122	16.873383	-0.056215	3.348244
265.151500	3729.814191	16.878387	-0.056211	3.344875
265.007161	3721.852529	16.883392	-0.056180	3.341522
264.980564	3713.881397	16.888397	-0.056171	3.338166
264.974735	3705.837270	16.893402	-0.056167	3.334777
264.984515	3697.854720	16.898407	-0.056165	3.331410
264.820007	3689.862060	16.903411	-0.056130	3.328030
264.702483	3681.858760	16.908416	-0.056104	3.324643
264.872735	3673.911675	16.913421	-0.056132	3.321287
264.570611	3665.932644	16.918426	-0.056072	3.317897
264.607876	3657.941853	16.923431	-0.056075	3.314511
264.507583	3649.918308	16.928435	-0.056053	3.311102
264.459011	3641.900742	16.933440	-0.056040	3.307694
264.286335	3633.928785	16.938445	-0.056004	3.304298
264.221324	3625.944629	16.943450	-0.055988	3.300897
264.353433	3617.959387	16.948455	-0.056009	3.297499
264.279399	3609.985922	16.953459	-0.055991	3.294095
263.928338	3601.976611	16.958464	-0.055922	3.290662
263.970779	3594.018965	16.963469	-0.055926	3.287262
263.957398	3585.999397	16.968474	-0.055920	3.283830
263.879290	3578.052270	16.973479	-0.055902	3.280423
263.884643	3570.076866	16.978483	-0.055899	3.277004
264.067466	3562.033543	16.983488	-0.055929	3.273558
263.966794	3554.021165	16.988493	-0.055906	3.270111
263.863184	3546.032054	16.993498	-0.055883	3.266671
263.908996	3538.061841	16.998503	-0.055888	3.263241
263.755687	3530.095552	17.003507	-0.055856	3.259801
263.500619	3522.152752	17.008512	-0.055804	3.256364
263.671210	3514.116245	17.013517	-0.055832	3.252899
263.586031	3506.071089	17.018522	-0.055813	3.249417
263.682049	3498.105285	17.023527	-0.055827	3.245972
263.649542	3490.138757	17.028531	-0.055817	3.242519
263.600440	3482.152765	17.033536	-0.055804	3.239052
263.482510	3474.198187	17.038541	-0.055778	3.235593
263.143945	3466.159076	17.043546	-0.055711	3.232084
263.340483	3458.126850	17.048551	-0.055744	3.228597
263.368865	3450.121605	17.053555	-0.055745	3.225110
263.357225	3442.165906	17.058560	-0.055739	3.221640
263.133928	3434.210551	17.063565	-0.055694	3.218157
263.146559	3426.207010	17.068570	-0.055693	3.214659
263.205222	3418.202894	17.073575	-0.055700	3.211159
263.128787	3410.196584	17.078579	-0.055682	3.207649
262.878948	3402.227392	17.083584	-0.055631	3.204143
262.988992	3394.288740	17.088589	-0.055648	3.200663
262.802631	3386.311972	17.093594	-0.055609	3.197149
262.933840	3378.307082	17.098599	-0.055630	3.193633
262.935362	3370.273593	17.103603	-0.055627	3.190094
262.768483	3362.314461	17.108608	-0.055592	3.186578
262.585616	3354.379847	17.113613	-0.055554	3.183067
262.511452	3346.346334	17.118618	-0.055536	3.179514
262.481635	3338.381793	17.123623	-0.055527	3.175989
262.294440	3330.366441	17.128627	-0.055488	3.172430
262.189768	3322.374105	17.133632	-0.055465	3.168882
262.176392	3314.390471	17.138637	-0.055459	3.165337
261.901342	3306.423326	17.143642	-0.055404	3.161785
262.017788	3298.407322	17.148647	-0.055421	3.158223
262.124050	3290.426498	17.153651	-0.055437	3.154673
261.978053	3282.392183	17.158656	-0.055406	3.151084
261.878280	3274.444392	17.163661	-0.055384	3.147531
261.864003	3266.411481	17.168666	-0.055377	3.143940
261.927382	3258.437392	17.173671	-0.055385	3.140375
261.750460	3250.503357	17.178675	-0.055349	3.136813
261.560406	3242.496220	17.183680	-0.055310	3.133214
261.943927	3234.462527	17.188685	-0.055377	3.129623
261.627378	3226.518150	17.193690	-0.055314	3.126038
261.527969	3218.571464	17.198695	-0.055292	3.122458
261.411436	3210.591998	17.203699	-0.055267	3.118858
261.564437	3202.580752	17.208704	-0.055291	3.115251
261.603692	3194.560215	17.213709	-0.055295	3.111630
261.518020	3186.566167	17.218714	-0.055275	3.108012
261.568797	3178.576921	17.223719	-0.055281	3.104398
261.587133	3170.620135	17.228723	-0.055280	3.100793
261.341283	3162.656215	17.233728	-0.055231	3.097169
261.428268	3154.643869	17.238733	-0.055243	3.093533
261.096767	3146.667561	17.243738	-0.055177	3.089891
261.199783	3138.671088	17.248743	-0.055193	3.086255
261.318179	3130.689290	17.253747	-0.055211	3.082622
261.297349	3122.694582	17.258752	-0.055203	3.078972
261.207525	3114.726543	17.263757	-0.055183	3.075327
261.052494	3106.668177	17.268762	-0.055150	3.071634
261.211935	3098.666168	17.273767	-0.055176	3.067976
260.981111	3090.698126	17.278771	-0.055129	3.064311
260.827711	3082.750233	17.283776	-0.055097	3.060655
260.500104	3074.843855	17.288781	-0.055032	3.057005
260.311399	3066.818390	17.293786	-0.054993	3.053303
260.663099	3058.751735	17.298791	-0.055055	3.049602
260.696825	3050.791405	17.303795	-0.055057	3.045932
260.572796	3042.820320	17.308800	-0.055030	3.042244
260.452630	3034.890947	17.313805	-0.055004	3.038571
260.448211	3026.893302	17.318810	-0.054999	3.034868
260.390217	3018.895455	17.323815	-0.054985	3.031157
260.405915	3010.883700	17.328819	-0.054984	3.027439
260.371184	3002.901083	17.333824	-0.054974	3.023728
260.323625	2994.938327	17.338829	-0.054961	3.020021
260.185555	2986.982033	17.343834	-0.054931	3.016307
260.182745	2978.958685	17.348839	-0.054927	3.012565
260.183052	2970.973040	17.353843	-0.054923	3.008835
260.033897	2962.987524	17.358848	-0.054892	3.005094
259.989910	2955.059681	17.363853	-0.054880	3.001380
259.778036	2947.066736	17.368858	-0.054837	2.997622
259.826140	2939.085243	17.373863	-0.054842	2.993878
259.642582	2931.093564	17.378867	-0.054804	2.990114
259.742222	2923.066329	17.383872	-0.054818	2.986341
259.798921	2915.106683	17.388877	-0.054825	2.982594
259.498436	2907.153734	17.393882	-0.054765	2.978827
259.500937	2899.139969	17.398887	-0.054762	2.975042
259.586682	2891.122956	17.403891	-0.054774	2.971255
259.501841	2883.123036	17.408896	-0.054755	2.967462
259.573993	2875.179843	17.413901	-0.054764	2.963700
259.516114	2867.163964	17.418906	-0.054750	2.959891
259.516538	2859.234893	17.423911	-0.054746	2.956122
259.326820	2851.258934	17.428915	-0.054707	2.952316
259.190814	2843.244400	17.433920	-0.054678	2.948489
259.376322	2835.242422	17.438925	-0.054708	2.944680
259.369891	2827.295503	17.443930	-0.054703	2.940882
259.321864	2819.324210	17.448935	-0.054691	2.937066
259.295284	2811.340798	17.453939	-0.054682	2.933240
259.249477	2803.334125	17.458944	-0.054670	2.929397
259.204144	2795.371702	17.463949	-0.054657	2.925570
259.036247	2787.403835	17.468954	-0.054622	2.921729
259.053331	2779.430302	17.473959	-0.054622	2.917890
258.996320	2771.443625	17.478963	-0.054607	2.914035
258.776000	2763.363908	17.483968	-0.054562	2.910122
258.943764	2755.386296	17.488973	-0.054590	2.906274
258.942121	2747.419027	17.493978	-0.054586	2.902416
258.810135	2739.468284	17.498983	-0.054557	2.898555
258.844957	2731.486735	17.503987	-0.054560	2.894682
258.758897	2723.506053	17.508992	-0.054540	2.890798
258.705965	2715.544021	17.513997	-0.054526	2.886919
258.337983	2707.593606	17.519002	-0.054454	2.883024
258.569417	2699.591613	17.524007	-0.054493	2.879131
258.312163	2691.644931	17.529011	-0.054442	2.875233
257.907906	2683.661748	17.534016	-0.054363	2.871304
257.884763	2675.721773	17.539021	-0.054354	2.867412
258.018201	2667.663892	17.544026	-0.054375	2.863465
257.776638	2659.702722	17.549031	-0.054327	2.859539
257.830004	2651.737369	17.554035	-0.054333	2.855622
257.691517	2643.727812	17.559040	-0.054303	2.851667
257.741938	2635.765758	17.564045	-0.054309	2.847741
257.799137	2627.738138	17.569050	-0.054316	2.843778
257.780544	2619.785687	17.574055	-0.054308	2.839841
257.650103	2611.849963	17.579059	-0.054280	2.835902
257.578163	2603.794878	17.584064	-0.054263	2.831901
257.722893	2595.826493	17.589069	-0.054286	2.827949
257.576682	2587.838219	17.594074	-0.054255	2.823966
257.575865	2579.874195	17.599079	-0.054251	2.819997
257.335110	2571.944309	17.604083	-0.054203	2.816026
257.016811	2563.983391	17.609088	-0.054140	2.812030
257.236078	2555.961974	17.614093	-0.054177	2.808028
257.085777	2547.951817	17.619098	-0.054145	2.804005
256.914969	2540.037628	17.624103	-0.054109	2.800023
257.033424	2532.038897	17.629107	-0.054127	2.796010
257.116248	2524.010434	17.634112	-0.054139	2.791974
257.006546	2516.062737	17.639117	-0.054115	2.787961
257.011296	2508.057716	17.644122	-0.054112	2.783921
256.971074	2500.109616	17.649127	-0.054101	2.779900
256.915109	2492.153287	17.654131	-0.054086	2.775869
257.107477	2484.122526	17.659136	-0.054118	2.771809
257.169764	2476.160919	17.664141	-0.054126	2.767771
256.741184	2468.218308	17.669146	-0.054042	2.763707
256.719885	2460.253016	17.674151	-0.054035	2.759649
256.912301	2452.275722	17.679155	-0.054067	2.755593
256.433839	2444.251082	17.684160	-0.053974	2.751466
256.395770	2436.279254	17.689165	-0.053963	2.747386
256.523673	2428.268147	17.694170	-0.053983	2.743290
256.523354	2420.326557	17.699175	-0.053979	2.739215
256.380161	2412.366845	17.704179	-0.053949	2.735117
256.177481	2404.389173	17.709184	-0.053907	2.731000
256.465754	2396.390480	17.714189	-0.053957	2.726895
256.262596	2388.429758	17.719194	-0.053915	2.722774
256.436828	2380.460623	17.724199	-0.053944	2.718666
256.293178	2372.496566	17.729203	-0.053913	2.714534
256.150505	2364.485635	17.734208	-0.053883	2.710372
256.282192	2356.538515	17.739213	-0.053904	2.706253
255.922005	2348.591898	17.744218	-0.053833	2.702098
255.875645	2340.623211	17.749223	-0.053820	2.697945
256.073212	2332.619093	17.754227	-0.053853	2.693782
255.840004	2324.658557	17.759232	-0.053806	2.689608
255.931892	2316.682806	17.764237	-0.053819	2.685440
255.643847	2308.738277	17.769242	-0.053762	2.681258
255.660146	2300.772027	17.774247	-0.053761	2.677077
255.847888	2292.745316	17.779251	-0.053792	2.672869
255.542515	2284.788930	17.784256	-0.053732	2.668660
255.350058	2276.839882	17.789261	-0.053692	2.664455
255.571767	2268.824353	17.794266	-0.053730	2.660235
255.301000	2260.905955	17.799271	-0.053675	2.656028
255.217432	2252.916864	17.804275	-0.053656	2.651789
255.089736	2244.908061	17.809280	-0.053628	2.647530
255.333967	2236.917593	17.814285	-0.053670	2.643298
255.205182	2228.987983	17.819290	-0.053642	2.639067
255.296122	2221.005962	17.824295	-0.053655	2.634816
255.316017	2213.007811	17.829299	-0.053655	2.630545
255.314715	2205.025233	17.834304	-0.053651	2.626273
255.140809	2197.097808	17.839309	-0.053615	2.622013
254.996212	2189.142275	17.844314	-0.053584	2.617733
255.135896	2181.156067	17.849319	-0.053607	2.613448
254.913155	2173.191733	17.854323	-0.053561	2.609144
254.649253	2165.243157	17.859328	-0.053508	2.604838
254.806550	2157.277319	17.864333	-0.053534	2.600544
254.780494	2149.308685	17.869338	-0.053525	2.596229
254.633953	2141.197427	17.874343	-0.053494	2.591821
254.748706	2133.156240	17.879347	-0.053512	2.587462
254.448805	2125.253339	17.884352	-0.053452	2.583142
254.517915	2117.340631	17.889357	-0.053461	2.578835
254.250974	2109.399705	17.894362	-0.053408	2.574482
254.438478	2101.396027	17.899367	-0.053439	2.570119
254.330056	2093.449502	17.904371	-0.053415	2.565759
254.197494	2085.498824	17.909376	-0.053386	2.561388
254.455147	2077.528278	17.914381	-0.053430	2.557026
254.159749	2069.573753	17.919386	-0.053372	2.552626
253.867073	2061.627396	17.924391	-0.053313	2.548224
253.847967	2053.664297	17.929395	-0.053306	2.543823
253.904010	2045.675307	17.934400	-0.053313	2.539406
253.806271	2037.737965	17.939405	-0.053291	2.535000
253.780939	2029.742091	17.944410	-0.053282	2.530558
253.804509	2021.756843	17.949415	-0.053283	2.526117
253.678321	2013.826242	17.954419	-0.053255	2.521689
253.599009	2005.871253	17.959424	-0.053237	2.517242
253.630217	1997.881655	17.964429	-0.053239	2.512776
253.465184	1989.896836	17.969434	-0.053204	2.508291
253.464510	1981.929492	17.974439	-0.053200	2.503820
253.508351	1973.968437	17.979443	-0.053205	2.499347
253.464945	1966.001807	17.984448	-0.053193	2.494856
253.380159	1958.046297	17.989453	-0.053173	2.490361
253.463445	1950.058137	17.994458	-0.053185	2.485851
253.314800	1942.128963	17.999463	-0.053153	2.481350
253.085775	1934.208440	18.004467	-0.053107	2.476840
253.195630	1926.189160	18.009472	-0.053124	2.472290
253.101616	1918.242781	18.014477	-0.053102	2.467758
253.091713	1910.262670	18.019482	-0.053097	2.463204
253.050173	1902.324071	18.024487	-0.053085	2.458664
252.884622	1894.374920	18.029491	-0.053051	2.454100
252.710906	1886.393060	18.034496	-0.053014	2.449508
252.715047	1878.449950	18.039501	-0.053011	2.444943
252.579653	1870.492268	18.044506	-0.052982	2.440351
252.713602	1862.527838	18.049511	-0.053004	2.435766
252.698357	1854.502126	18.054515	-0.052997	2.431126
252.546098	1846.519983	18.059520	-0.052965	2.426492
252.647912	1838.575074	18.064525	-0.052980	2.421890
252.368967	1830.658124	18.069530	-0.052924	2.417266
252.290959	1822.682291	18.074535	-0.052906	2.412615
252.335471	1814.716624	18.079539	-0.052910	2.407970
252.101688	1806.770619	18.084544	-0.052863	2.403305
252.159304	1798.826002	18.089549	-0.052870	2.398656
252.052353	1790.863617	18.094554	-0.052846	2.393974
252.145194	1782.869865	18.099559	-0.052860	2.389280
251.964200	1774.924004	18.104563	-0.052822	2.384583
251.723991	1767.002597	18.109568	-0.052774	2.379887
251.787405	1759.055862	18.114573	-0.052782	2.375190
251.656032	1751.064847	18.119578	-0.052753	2.370443
251.781994	1743.099259	18.124583	-0.052773	2.365722
251.777545	1735.155192	18.129587	-0.052768	2.360993
251.803602	1727.200180	18.134592	-0.052770	2.356251
251.658813	1719.254925	18.139597	-0.052739	2.351492
251.625404	1711.261346	18.144602	-0.052729	2.346702
251.646523	1703.302717	18.149607	-0.052729	2.341929
251.494459	1695.392256	18.154611	-0.052697	2.337160
251.244415	1687.421487	18.159616	-0.052646	2.332338
251.287170	1679.456323	18.164621	-0.052651	2.327533
251.231925	1671.503859	18.169626	-0.052637	2.322717
251.155633	1663.561769	18.174631	-0.052619	2.317896
251.053384	1655.625655	18.179635	-0.052596	2.313067
251.181387	1647.615863	18.184640	-0.052616	2.308201
251.128359	1639.696394	18.189645	-0.052602	2.303365
250.954297	1631.760903	18.194650	-0.052566	2.298500
251.105661	1623.783499	18.199655	-0.052590	2.293625
251.086285	1615.822732	18.204659	-0.052583	2.288736
250.836477	1607.889330	18.209664	-0.052533	2.283834
250.853487	1599.966764	18.214669	-0.052532	2.278950
250.683442	1592.006420	18.219674	-0.052497	2.274017
250.736996	1583.972440	18.224679	-0.052503	2.269047
250.662306	1576.029238	18.229683	-0.052485	2.264111
250.689530	1568.085287	18.234688	-0.052486	2.259172
250.630859	1560.161060	18.239693	-0.052472	2.254228
250.487182	1552.197399	18.244698	-0.052441	2.249240
250.444117	1544.260667	18.249703	-0.052429	2.244267
250.423302	1536.336455	18.254707	-0.052422	2.239293
250.088547	1528.414070	18.259712	-0.052355	2.234282
250.194214	1520.431185	18.264717	-0.052371	2.229259
250.087399	1512.482052	18.269722	-0.052348	2.224228
250.001255	1504.555455	18.274727	-0.052328	2.219202
249.886968	1496.630407	18.279731	-0.052303	2.214162
249.828914	1488.656996	18.284736	-0.052288	2.209086
249.890769	1480.706370	18.289741	-0.052296	2.204023
249.635315	1472.799297	18.294746	-0.052245	2.198947
249.676221	1464.838722	18.299751	-0.052248	2.193852
249.708291	1456.864809	18.304755	-0.052251	2.188736
249.370583	1448.940148	18.309760	-0.052184	2.183606
249.793943	1440.961519	18.314765	-0.052259	2.178499
249.666140	1433.020721	18.319770	-0.052231	2.173354
249.820884	1425.043099	18.324775	-0.052256	2.168198
249.525238	1417.174664	18.329779	-0.052198	2.163060
249.340230	1409.252884	18.334784	-0.052159	2.157884
249.510637	1401.276451	18.339789	-0.052187	2.152694
249.298004	1393.335593	18.344794	-0.052144	2.147479
249.109035	1385.422901	18.349799	-0.052105	2.142271
249.037717	1377.504210	18.354803	-0.052088	2.137059
248.906020	1369.545866	18.359808	-0.052060	2.131801
248.930918	1361.592803	18.364813	-0.052060	2.126549
248.883180	1353.666241	18.369818	-0.052048	2.121294
248.615715	1345.762504	18.374823	-0.051994	2.116020
248.693907	1337.747636	18.379827	-0.052005	2.110693
248.666161	1329.775429	18.384832	-0.051996	2.105370
248.662895	1321.859921	18.389837	-0.051992	2.100074
248.549454	1313.955177	18.394842	-0.051967	2.094761
248.447526	1306.017186	18.399847	-0.051944	2.089413
248.638871	1298.053837	18.404851	-0.051976	2.084063
248.538407	1290.146644	18.409856	-0.051953	2.078709
248.546111	1282.225757	18.414861	-0.051951	2.073342
248.472174	1274.269538	18.419866	-0.051933	2.067930
248.336514	1266.358045	18.424871	-0.051904	2.062527
248.432103	1258.432714	18.429875	-0.051918	2.057124
248.168001	1250.518723	18.434880	-0.051865	2.051678
248.089504	1242.592872	18.439885	-0.051847	2.046228
247.993378	1234.673543	18.444890	-0.051825	2.040767
247.729944	1226.778315	18.449895	-0.051773	2.035290
247.888099	1218.777083	18.454899	-0.051798	2.029768
247.696989	1210.854656	18.459904	-0.051759	2.024250
247.800562	1202.931176	18.464909	-0.051774	2.018746
247.724390	1194.999625	18.469914	-0.051756	2.013204
247.834153	1187.051588	18.474919	-0.051773	2.007653
247.597073	1179.156904	18.479923	-0.051725	2.002089
247.317929	1171.273937	18.484928	-0.051669	1.996513
247.458441	1163.313230	18.489933	-0.051692	1.990910
247.394076	1155.376771	18.494938	-0.051676	1.985287
247.364951	1147.469220	18.499943	-0.051667	1.979673
247.207767	1139.576861	18.504947	-0.051634	1.974039
247.047653	1131.638774	18.509952	-0.051600	1.968357
246.894720	1123.744627	18.514957	-0.051568	1.962690
246.906302	1115.816016	18.519962	-0.051566	1.957000
247.153958	1107.819919	18.524967	-0.051609	1.951270
247.058731	1099.898192	18.529971	-0.051587	1.945539
246.809493	1092.011529	18.534976	-0.051537	1.939801
246.811900	1084.107166	18.539981	-0.051534	1.934060
246.650787	1076.169950	18.544986	-0.051500	1.928260
246.738460	1068.245716	18.549991	-0.051512	1.922479
246.770525	1060.355710	18.554995	-0.051515	1.916700
246.677883	1052.429180	18.560000	-0.051494	1.910862
246.380037	1044.545231	18.565005	-0.051434	1.905016
246.350523	1036.644054	18.570010	-0.051425	1.899168
246.330626	1028.734866	18.575015	-0.051418	1.893298
246.249928	1020.823809	18.580019	-0.051399	1.887401
246.195662	1012.906149	18.585024	-0.051385	1.881483
246.245514	1005.009223	18.590029	-0.051391	1.875575
246.201831	997.076670	18.595034	-0.051379	1.869610
245.978822	989.181462	18.600039	-0.051333	1.863633
245.987681	981.274901	18.605043	-0.051331	1.857656
245.704587	973.390284	18.610048	-0.051275	1.851642
245.903357	965.461651	18.615053	-0.051308	1.845630
245.625843	957.599758	18.620058	-0.051253	1.839595
245.439633	949.714469	18.625063	-0.051214	1.833532
245.613033	941.766092	18.630067	-0.051243	1.827444
245.217028	933.902873	18.635072	-0.051165	1.821333
245.517843	925.965911	18.640077	-0.051217	1.815227
245.520788	918.064929	18.645082	-0.051214	1.809093
245.443433	910.171885	18.650087	-0.051196	1.802935
245.366321	902.306989	18.655091	-0.051178	1.796777
245.130425	894.380821	18.660096	-0.051130	1.790531
245.040840	886.486727	18.665101	-0.051110	1.784306
244.773236	878.630271	18.670106	-0.051056	1.778068
244.819860	870.712291	18.675111	-0.051061	1.771797
244.836419	862.813799	18.680115	-0.051061	1.765516
244.660359	854.955579	18.685120	-0.051024	1.759220
244.720578	847.060764	18.690125	-0.051031	1.752902
244.593912	839.169221	18.695130	-0.051004	1.746540
244.436111	831.296304	18.700135	-0.050971	1.740166
244.443591	823.424541	18.705139	-0.050969	1.733791
244.386061	815.518462	18.710144	-0.050954	1.727356
244.381425	807.657789	18.715149	-0.050950	1.720940
244.212033	799.802989	18.720154	-0.050914	1.714485
244.384298	791.856896	18.725159	-0.050943	1.707973
244.401904	783.988814	18.730163	-0.050942	1.701482
244.041838	776.164522	18.735168	-0.050871	1.694952
244.048671	768.275500	18.740173	-0.050869	1.688391
244.000472	760.405804	18.745178	-0.050856	1.681814
243.642536	752.594322	18.750183	-0.050786	1.675218
243.711314	744.694114	18.755187	-0.050795	1.668579
243.781312	736.789808	18.760192	-0.050804	1.661909
243.626049	728.962589	18.765197	-0.050772	1.655248
243.502674	721.096615	18.770202	-0.050745	1.648531
243.467067	713.222196	18.775207	-0.050735	1.641792
243.481524	705.370466	18.780211	-0.050733	1.635051
243.290903	697.465446	18.785216	-0.050694	1.628207
243.228581	689.626526	18.790221	-0.050679	1.621410
243.302701	681.749574	18.795226	-0.050689	1.614570
243.226568	673.896733	18.800231	-0.050671	1.607702
243.135057	666.073529	18.805235	-0.050650	1.600827
242.931768	658.247610	18.810240	-0.050609	1.593905
242.588021	650.439144	18.815245	-0.050541	1.586947
242.576364	642.570775	18.820250	-0.050535	1.579954
242.733780	634.690573	18.825255	-0.050561	1.572943
242.570168	626.876002	18.830259	-0.050527	1.565913
242.421048	619.045345	18.835264	-0.050495	1.558838
242.341608	611.208926	18.840269	-0.050477	1.551737
242.253406	603.361313	18.845274	-0.050456	1.544591
242.222797	595.526025	18.850279	-0.050447	1.537432
242.057234	587.707312	18.855283	-0.050412	1.530235
242.018325	579.863015	18.860288	-0.050401	1.522999
242.220140	572.014786	18.865293	-0.050435	1.515761
241.986618	564.211337	18.870298	-0.050388	1.508464
241.904438	556.387020	18.875303	-0.050369	1.501134
241.806753	548.599132	18.880307	-0.050347	1.493801
241.699507	540.765492	18.885312	-0.050324	1.486387
241.720909	532.958120	18.890317	-0.050324	1.478981
241.635060	525.126492	18.895322	-0.050304	1.471497
241.530222	517.301277	18.900327	-0.050281	1.463979
241.381021	509.523719	18.905331	-0.050250	1.456460
241.279587	501.721331	18.910336	-0.050227	1.448886
241.336951	493.908689	18.915341	-0.050234	1.441287
241.280989	486.123600	18.920346	-0.050220	1.433657
241.117737	478.325790	18.925351	-0.050186	1.425956
241.045879	470.561549	18.930355	-0.050169	1.418262
240.945063	462.762374	18.935360	-0.050146	1.410486
240.917503	454.991288	18.940365	-0.050137	1.402707
240.790763	447.226113	18.945370	-0.050110	1.394874
240.589564	439.446788	18.950375	-0.050069	1.386970
240.465986	431.691094	18.955379	-0.050042	1.379058
240.380407	423.909902	18.960384	-0.050023	1.371080
240.386564	416.138898	18.965389	-0.050020	1.363082
240.283462	408.386616	18.970394	-0.049997	1.355037
240.215608	400.608603	18.975399	-0.049981	1.346923
240.141161	392.872631	18.980403	-0.049963	1.338804
239.964320	385.125095	18.985408	-0.049927	1.330604
239.973337	377.375526	18.990413	-0.049925	1.322384
239.860639	369.625199	18.995418	-0.049900	1.314091
239.911358	361.757652	19.000423	-0.049906	1.305647
239.654400	354.085425	19.005427	-0.049855	1.297305
239.613538	346.342795	19.010432	-0.049843	1.288871
239.554905	338.639726	19.015437	-0.049829	1.280422
239.299433	330.962380	19.020442	-0.049778	1.271909
239.137706	323.252725	19.025447	-0.049744	1.263319
239.357783	315.516262	19.030451	-0.049781	1.254713
239.110247	307.832070	19.035456	-0.049731	1.246018
239.055121	300.159941	19.040461	-0.049718	1.237312
239.026090	292.442574	19.045466	-0.049708	1.228497
238.918120	284.763651	19.050471	-0.049685	1.219648
238.736104	277.109814	19.055475	-0.049647	1.210748
238.708419	269.427043	19.060480	-0.049639	1.201780
238.699088	261.762464	19.065485	-0.049633	1.192769
238.554967	254.105359	19.070490	-0.049603	1.183671
238.439869	246.471822	19.075495	-0.049578	1.174536
238.347468	238.828212	19.080499	-0.049557	1.165323
238.249949	231.202171	19.085504	-0.049535	1.156056
238.019048	223.555595	19.090509	-0.049489	1.146661
237.935963	215.937480	19.095514	-0.049470	1.137256
237.801722	208.316799	19.100519	-0.049441	1.127757
237.737311	200.722615	19.105523	-0.049425	1.118226
237.468489	193.139234	19.110528	-0.049372	1.108582
237.507445	185.533681	19.115533	-0.049376	1.098893
237.248546	177.982096	19.120538	-0.049324	1.089121
236.927392	170.447483	19.125543	-0.049260	1.079269
237.096743	162.840019	19.130547	-0.049288	1.069341
236.721439	155.320260	19.135552	-0.049215	1.059312
236.416174	147.812051	19.140557	-0.049155	1.049218
236.216172	140.297097	19.145562	-0.049114	1.039042
235.913028	132.796656	19.150567	-0.049054	1.028761
235.901920	125.272872	19.155571	-0.049048	1.018413
235.648638	117.785741	19.160576	-0.048998	1.007951
235.633849	110.295722	19.165581	-0.048992	0.997435
235.416154	102.798301	19.170586	-0.048948	0.986745
235.292122	95.337145	19.175591	-0.048921	0.976013
235.153540	87.893597	19.180595	-0.048892	0.965184
234.548116	80.544072	19.185600	-0.048776	0.954251
234.095766	73.172655	19.190605	-0.048688	0.943198
233.666489	65.818732	19.195610	-0.048605	0.932046
233.400619	58.679567	19.200615	-0.048552	0.921131