Tue Mar 23 10:20:28 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.624219	0.027207	0.000000	0.000037	0.729338

0.431146	0.065756	0.005005	0.000072	0.729347
0.457283	0.058878	0.010010	0.000067	0.729343
0.387942	0.071758	0.015014	0.000079	0.729345
0.401088	0.069680	0.020019	0.000076	0.729347
0.106544	0.116931	0.025024	0.000130	0.729337
0.381138	0.071945	0.030029	0.000079	0.729346
0.416646	-0.037459	0.035034	0.000072	0.729146
0.453369	-0.102918	0.040038	0.000065	0.729033
0.376113	-0.087948	0.045043	0.000078	0.729036
0.525356	-0.117453	0.050048	0.000050	0.729031
0.527888	-0.114754	0.055053	0.000049	0.729038
0.350200	-0.084722	0.060058	0.000082	0.729036
0.337567	-0.081571	0.065062	0.000084	0.729038
0.450129	-0.101460	0.070067	0.000062	0.729040
0.436765	-0.103636	0.075072	0.000064	0.729032
0.730604	-0.153133	0.080077	0.000009	0.729038
0.449685	-0.107099	0.085082	0.000061	0.729031
0.379617	-0.094772	0.090086	0.000073	0.729032
0.345339	-0.197851	0.095091	0.000079	0.728820
0.331649	-0.250825	0.100096	0.000082	0.728713
0.295538	-0.239848	0.105101	0.000088	0.728723
0.300612	-0.243177	0.110106	0.000086	0.728719
0.350072	-0.253723	0.115110	0.000077	0.728717
0.313591	-0.243763	0.120115	0.000083	0.728725
0.255306	-0.243800	0.125120	0.000093	0.728705
0.380121	-0.414068	0.130125	0.000070	0.728418
0.235158	-0.388734	0.135130	0.000096	0.728418
0.234302	-0.389484	0.140134	0.000096	0.728417
0.390770	-0.414461	0.145139	0.000066	0.728423
0.453179	-0.435569	0.150144	0.000054	0.728405
0.604105	-0.625691	0.155149	0.000026	0.728088
0.342347	-0.580976	0.160154	0.000074	0.728085
0.505804	-0.611687	0.165158	0.000043	0.728083
0.397864	-0.588372	0.170163	0.000063	0.728092
0.193688	-0.711509	0.175168	0.000100	0.727782
0.321139	-0.736613	0.180173	0.000076	0.727778
0.381372	-0.748955	0.185178	0.000064	0.727776
0.291967	-0.771435	0.190182	0.000081	0.727702
0.395769	-0.915063	0.195187	0.000061	0.727459
0.358565	-0.911666	0.200192	0.000067	0.727454
0.343861	-0.905187	0.205197	0.000070	0.727462
0.341242	-1.043163	0.210202	0.000070	0.727193
0.307973	-1.057434	0.215206	0.000075	0.727154
0.191504	-1.033767	0.220211	0.000097	0.727161
0.126110	-1.151792	0.225216	0.000108	0.726909
0.246298	-1.212047	0.230221	0.000086	0.726834
0.315381	-1.225483	0.235226	0.000072	0.726833
0.316538	-1.357893	0.240230	0.000072	0.726576
0.258616	-1.370918	0.245235	0.000082	0.726531
0.095253	-1.361779	0.250240	0.000112	0.726493
0.307580	-1.542380	0.255245	0.000072	0.726215
0.195951	-1.525133	0.260250	0.000092	0.726211
0.343252	-1.624784	0.265254	0.000064	0.726068
0.306464	-1.685106	0.270259	0.000071	0.725939
0.162316	-1.675494	0.275264	0.000097	0.725908
0.138708	-1.827249	0.280269	0.000101	0.725604
-0.142617	-1.778479	0.285274	0.000153	0.725603
-0.104237	-1.892739	0.290278	0.000145	0.725394
0.082086	-1.978098	0.295283	0.000110	0.725292
-0.180576	-1.987410	0.300288	0.000159	0.725184
-0.038794	-2.120212	0.305293	0.000132	0.724974
-0.159572	-2.109191	0.310298	0.000154	0.724955
-0.084063	-2.271643	0.315302	0.000140	0.724664
-0.159334	-2.253203	0.320307	0.000153	0.724675
-0.386486	-2.366749	0.325312	0.000195	0.724374
-0.562157	-2.350573	0.330317	0.000227	0.724346
-1.001314	-2.382356	0.335322	0.000308	0.724131
-3.016479	-2.071261	0.340326	0.000683	0.724039
-2.490984	-2.162710	0.345331	0.000585	0.724044
-3.185077	-2.184153	0.350336	0.000713	0.723761
-3.752060	-2.107068	0.355341	0.000819	0.723715
-3.688982	-2.120869	0.360346	0.000806	0.723711
-3.659444	-2.208781	0.365350	0.000800	0.723550
-4.575637	-2.121479	0.370355	0.000970	0.723402
-4.627413	-2.118577	0.375360	0.000980	0.723391
-4.544455	-2.129267	0.380365	0.000964	0.723399
-5.111223	-2.180914	0.385370	0.001069	0.723101
-6.014582	-2.055382	0.390374	0.001236	0.723033
-5.750583	-2.098860	0.395379	0.001187	0.723041
-6.097378	-2.044630	0.400384	0.001251	0.723027
-5.794988	-2.136000	0.405389	0.001194	0.722954
-6.479778	-2.135755	0.410394	0.001321	0.722716
-6.752271	-2.090771	0.415398	0.001371	0.722710
-6.967865	-2.050229	0.420403	0.001411	0.722716
-6.857199	-2.076953	0.425408	0.001390	0.722703
-6.544250	-2.168914	0.430413	0.001331	0.722632
-7.867346	-2.064637	0.435418	0.001577	0.722376
-7.918637	-2.056048	0.440422	0.001586	0.722375
-7.493065	-2.127302	0.445427	0.001506	0.722385
-7.703877	-2.094408	0.450432	0.001545	0.722377
-8.196960	-2.002719	0.455437	0.001636	0.722386
-8.005126	-2.091704	0.460442	0.001600	0.722279
-8.764294	-2.057512	0.465446	0.001741	0.722081
-8.583843	-2.086721	0.470451	0.001707	0.722088
-8.981560	-2.022220	0.475456	0.001781	0.722077
-8.820916	-2.046274	0.480461	0.001750	0.722086
-8.562409	-2.094783	0.485466	0.001702	0.722082
-8.846299	-2.066239	0.490470	0.001754	0.722040
-9.277280	-2.133368	0.495475	0.001834	0.721758
-9.688279	-2.066101	0.500480	0.001910	0.721748
-9.680390	-2.065267	0.505485	0.001908	0.721753
-9.367175	-2.122721	0.510490	0.001849	0.721751
-9.700665	-2.064448	0.515494	0.001911	0.721749
-9.846441	-2.036098	0.520499	0.001937	0.721755
-10.010777	-2.116496	0.525504	0.001967	0.721540
-10.332968	-2.105250	0.530509	0.002027	0.721451
-10.485801	-2.080726	0.535514	0.002055	0.721446
-10.731086	-2.038789	0.540518	0.002100	0.721444
-10.380241	-2.096989	0.545523	0.002034	0.721453
-10.312917	-2.114161	0.550528	0.002021	0.721444
-10.475470	-2.121128	0.555533	0.002051	0.721374
-11.522901	-2.058170	0.560538	0.002246	0.721132
-11.375096	-2.087446	0.565542	0.002218	0.721127
-11.525231	-2.057013	0.570547	0.002245	0.721135
-11.920549	-1.993204	0.575552	0.002318	0.721123
-11.546946	-2.053594	0.580557	0.002248	0.721136
-11.357200	-2.092361	0.585562	0.002212	0.721127
-11.593209	-2.051003	0.590566	0.002256	0.721127
-11.707290	-2.144769	0.595571	0.002277	0.720903
-12.402203	-2.029204	0.600576	0.002405	0.720888
-12.503435	-2.008112	0.605581	0.002424	0.720895
-12.012495	-2.098004	0.610586	0.002332	0.720891
-12.089567	-2.087005	0.615590	0.002346	0.720887
-12.424854	-2.025154	0.620595	0.002408	0.720892
-12.587647	-2.031970	0.625600	0.002438	0.720822
-12.710050	-2.149735	0.630605	0.002460	0.720549
-12.692702	-2.155862	0.635610	0.002456	0.720543
-13.215811	-2.063386	0.640614	0.002553	0.720543
-12.926901	-2.111679	0.645619	0.002499	0.720550
-12.871874	-2.125942	0.650624	0.002488	0.720542
-13.372368	-2.033052	0.655629	0.002581	0.720551
-13.685727	-2.095759	0.660634	0.002639	0.720318
-14.413802	-2.014299	0.665638	0.002774	0.720224
-13.923218	-2.097037	0.670643	0.002682	0.720234
-14.106491	-2.068434	0.675648	0.002716	0.720227
-14.363232	-2.018785	0.680653	0.002763	0.720236
-14.021656	-2.084145	0.685658	0.002699	0.720228
-14.164194	-2.057287	0.690662	0.002725	0.720232
-13.967017	-2.154309	0.695667	0.002688	0.720111
-15.136765	-2.051943	0.700672	0.002905	0.719903
-15.098762	-2.052676	0.705677	0.002897	0.719916
-15.211059	-2.038450	0.710682	0.002918	0.719905
-15.209017	-2.038998	0.715686	0.002917	0.719906
-14.862334	-2.097544	0.720691	0.002852	0.719913
-15.417978	-2.002954	0.725696	0.002955	0.719905
-14.922627	-2.091852	0.730701	0.002862	0.719905
-15.460538	-2.147126	0.735706	0.002962	0.719608
-16.192961	-2.019392	0.740710	0.003098	0.719604
-16.137113	-2.025839	0.745715	0.003087	0.719611
-15.850456	-2.080668	0.750720	0.003033	0.719605
-15.813732	-2.083908	0.755725	0.003026	0.719612
-16.358891	-1.990151	0.760730	0.003127	0.719607
-16.216119	-2.017578	0.765734	0.003100	0.719604
-16.083743	-2.121372	0.770739	0.003075	0.719446
-17.356387	-1.980788	0.775744	0.003311	0.719278
-16.784012	-2.082138	0.780749	0.003204	0.719280
-17.081614	-2.029293	0.785754	0.003259	0.719280
-17.481724	-1.960449	0.790758	0.003333	0.719276
-16.823471	-2.072937	0.795763	0.003210	0.719287
-17.033999	-2.042797	0.800768	0.003249	0.719273
-17.332566	-1.987405	0.805773	0.003304	0.719278
-17.266443	-2.112357	0.810778	0.003291	0.719056
-18.053705	-2.019349	0.815782	0.003437	0.718964
-17.484158	-2.118221	0.820787	0.003331	0.718970
-17.710459	-2.084003	0.825792	0.003372	0.718959
-17.636963	-2.093281	0.830797	0.003358	0.718967
-17.718608	-2.080193	0.835802	0.003373	0.718965
-18.082027	-2.017881	0.840806	0.003440	0.718961
-18.244524	-2.102546	0.845811	0.003470	0.718738
-18.916720	-2.030003	0.850816	0.003594	0.718646
-18.650410	-2.075396	0.855821	0.003544	0.718651
-18.651954	-2.075820	0.860826	0.003544	0.718650
-18.706514	-2.068108	0.865830	0.003554	0.718647
-18.480271	-2.105932	0.870835	0.003511	0.718653
-18.672813	-2.075943	0.875840	0.003547	0.718645
-19.115322	-2.097612	0.880845	0.003628	0.718448
-19.591697	-2.057309	0.885850	0.003717	0.718361
-19.709004	-2.039608	0.890854	0.003738	0.718356
-19.485157	-2.074913	0.895859	0.003696	0.718365
-19.665860	-2.046871	0.900864	0.003729	0.718358
-19.538278	-2.068274	0.905869	0.003705	0.718362
-19.871115	-2.010494	0.910874	0.003766	0.718360
-19.942272	-2.055856	0.915878	0.003779	0.718246
-20.371482	-2.090694	0.920883	0.003858	0.718027
-20.409155	-2.085158	0.925888	0.003865	0.718026
-20.800068	-2.015020	0.930893	0.003937	0.718028
-20.596896	-2.052690	0.935898	0.003899	0.718026
-20.219549	-2.122797	0.940902	0.003828	0.718021
-20.658938	-2.041578	0.945907	0.003910	0.718028
-20.654600	-2.069393	0.950912	0.003908	0.717975
-20.990351	-2.142702	0.955917	0.003970	0.717713
-21.322426	-2.084265	0.960922	0.004032	0.717712
-21.737534	-2.012896	0.965926	0.004108	0.717708
-21.165640	-2.108766	0.970931	0.004002	0.717721
-21.296525	-2.092474	0.975936	0.004025	0.717708
-21.775733	-2.003295	0.980941	0.004114	0.717716
-21.406168	-2.085440	0.985946	0.004045	0.717685
-22.191735	-2.096581	0.990950	0.004191	0.717387
-22.346161	-2.065912	0.995955	0.004219	0.717395
-22.857292	-1.980439	1.000960	0.004314	0.717384
-22.438015	-2.052332	1.005965	0.004235	0.717391
-22.530037	-2.039485	1.010970	0.004252	0.717385
-22.743315	-2.002991	1.015974	0.004291	0.717383
-22.198783	-2.096480	1.020979	0.004189	0.717391
-22.524908	-2.102824	1.025984	0.004249	0.717264
-23.637205	-1.992183	1.030989	0.004456	0.717092
-23.204932	-2.070220	1.035994	0.004375	0.717091
-23.257886	-2.062513	1.040998	0.004384	0.717088
-23.347593	-2.044042	1.046003	0.004401	0.717094
-23.567350	-2.008957	1.051008	0.004441	0.717087
-23.254408	-2.063178	1.056013	0.004382	0.717091
-23.253508	-2.066009	1.061018	0.004382	0.717087
-24.323100	-2.042790	1.066022	0.004580	0.716756
-24.013921	-2.094452	1.071027	0.004522	0.716764
-24.273314	-2.051359	1.076032	0.004570	0.716759
-24.282782	-2.046744	1.081037	0.004571	0.716766
-24.469581	-2.013781	1.086042	0.004606	0.716766
-24.498792	-2.011919	1.091046	0.004610	0.716760
-24.186713	-2.064017	1.096051	0.004552	0.716768
-24.663609	-2.039507	1.101056	0.004640	0.716649
-25.387452	-2.008089	1.106061	0.004775	0.716457
-24.873049	-2.101189	1.111066	0.004678	0.716455
-25.203420	-2.044271	1.116070	0.004739	0.716452
-25.065507	-2.066497	1.121075	0.004713	0.716458
-25.139262	-2.058118	1.126080	0.004726	0.716449
-25.113375	-2.058383	1.131085	0.004721	0.716459
-25.020340	-2.123251	1.136090	0.004703	0.716364
-25.767758	-2.106105	1.141094	0.004842	0.716135
-25.822144	-2.091564	1.146099	0.004852	0.716146
-26.637126	-1.952903	1.151104	0.005003	0.716134
-25.938392	-2.074423	1.156109	0.004872	0.716140
-25.814963	-2.098365	1.161114	0.004849	0.716137
-26.475181	-1.983329	1.166118	0.004971	0.716133
-26.250995	-2.026751	1.171123	0.004929	0.716127
-26.409741	-2.122045	1.176128	0.004958	0.715883
-26.755005	-2.057904	1.181133	0.005022	0.715889
-26.857509	-2.041212	1.186138	0.005041	0.715887
-26.540692	-2.100659	1.191142	0.004981	0.715882
-26.485700	-2.106900	1.196147	0.004970	0.715890
-26.936009	-2.031412	1.201152	0.005054	0.715882
-26.763356	-2.159510	1.206157	0.005021	0.715690
-27.762273	-2.051959	1.211162	0.005207	0.715551
-28.069540	-1.999701	1.216166	0.005263	0.715547
-27.511291	-2.096955	1.221171	0.005159	0.715552
-27.689528	-2.069056	1.226176	0.005192	0.715546
-27.674309	-2.069356	1.231181	0.005188	0.715551
-27.533250	-2.095847	1.236186	0.005162	0.715549
-27.838294	-2.144442	1.241190	0.005218	0.715346
-28.482547	-2.082006	1.246195	0.005337	0.715243
-28.661359	-2.057346	1.251200	0.005370	0.715230
-28.363856	-2.108476	1.256205	0.005314	0.715235
-28.524089	-2.080123	1.261210	0.005344	0.715235
-28.867513	-2.020519	1.266214	0.005407	0.715233
-28.559058	-2.070138	1.271219	0.005349	0.715244
-28.556010	-2.191454	1.276224	0.005348	0.715006
-29.651121	-2.041646	1.281229	0.005552	0.714917
-29.661533	-2.041591	1.286234	0.005553	0.714914
-29.403391	-2.090352	1.291238	0.005504	0.714910
-29.423673	-2.083427	1.296243	0.005508	0.714917
-29.647366	-2.047663	1.301248	0.005549	0.714910
-29.544157	-2.063009	1.306253	0.005529	0.714917
-29.555362	-2.152406	1.311258	0.005531	0.714736
-30.616304	-2.027645	1.316262	0.005728	0.714610
-30.492938	-2.044028	1.321267	0.005704	0.714622
-30.648506	-2.021222	1.326272	0.005733	0.714613
-30.725133	-2.005481	1.331277	0.005747	0.714618
-30.386669	-2.066662	1.336282	0.005683	0.714617
-30.548941	-2.039871	1.341286	0.005713	0.714614
-30.451047	-2.074747	1.346291	0.005694	0.714580
-31.373704	-2.062601	1.351296	0.005866	0.714279
-31.385338	-2.057377	1.356301	0.005867	0.714286
-31.574162	-2.021259	1.361306	0.005902	0.714292
-31.936160	-1.959047	1.366310	0.005969	0.714288
-31.947329	-1.948171	1.371315	0.005970	0.714307
-31.697683	-2.003118	1.376320	0.005923	0.714287
-31.351622	-2.064475	1.381325	0.005859	0.714288
-31.318622	-2.095523	1.386330	0.005852	0.714239
-32.519255	-2.015328	1.391334	0.006075	0.713974
-31.984163	-2.107375	1.396339	0.005975	0.713982
-32.419826	-2.034120	1.401344	0.006055	0.713974
-32.616644	-1.995990	1.406349	0.006092	0.713981
-32.489745	-2.020666	1.411354	0.006068	0.713978
-32.474940	-2.027338	1.416358	0.006064	0.713971
-32.389765	-2.035316	1.421363	0.006048	0.713986
-32.728480	-2.092470	1.426368	0.006111	0.713753
-33.393671	-2.019027	1.431373	0.006234	0.713665
-33.501148	-1.999990	1.436378	0.006253	0.713665
-33.206533	-2.057799	1.441382	0.006198	0.713656
-33.261157	-2.043665	1.446387	0.006208	0.713665
-33.758089	-1.959963	1.451392	0.006300	0.713657
-33.657711	-1.975716	1.456397	0.006281	0.713662
-33.350504	-2.037377	1.461402	0.006223	0.713649
-34.263283	-2.017827	1.466406	0.006392	0.713365
-34.516801	-1.967676	1.471411	0.006439	0.713376
-34.702308	-1.943448	1.476416	0.006473	0.713360
-34.305448	-2.006524	1.481421	0.006399	0.713376
-34.369395	-1.998381	1.486426	0.006410	0.713370
-34.603562	-1.960150	1.491430	0.006453	0.713364
-34.059899	-2.053299	1.496435	0.006352	0.713372
-34.352432	-2.056645	1.501440	0.006406	0.713263
-35.357753	-1.992452	1.506445	0.006592	0.713035
-34.887343	-2.078556	1.511450	0.006504	0.713032
-35.230148	-2.021480	1.516454	0.006568	0.713025
-35.337715	-1.996546	1.521459	0.006587	0.713037
-35.252937	-2.017364	1.526464	0.006571	0.713027
-35.160633	-2.031721	1.531469	0.006553	0.713032
-35.106254	-2.066767	1.536474	0.006543	0.712982
-35.933032	-2.053416	1.541478	0.006696	0.712716
-35.873331	-2.060516	1.546483	0.006685	0.712724
-36.347423	-1.980989	1.551488	0.006772	0.712715
-36.432851	-1.964822	1.556493	0.006788	0.712718
-36.011189	-2.041734	1.561498	0.006709	0.712715
-36.432712	-1.966398	1.566502	0.006787	0.712717
-36.233420	-2.000835	1.571507	0.006749	0.712720
-36.438095	-2.075493	1.576512	0.006787	0.712500
-37.133514	-2.003388	1.581517	0.006916	0.712397
-36.948212	-2.037566	1.586522	0.006881	0.712396
-37.348240	-1.966881	1.591526	0.006955	0.712396
-36.872295	-2.048568	1.596531	0.006866	0.712403
-36.806123	-2.066694	1.601536	0.006853	0.712391
-37.040241	-2.025723	1.606541	0.006896	0.712390
-37.046544	-2.103946	1.611546	0.006897	0.712233
-37.843073	-2.031739	1.616550	0.007044	0.712095
-37.505183	-2.088912	1.621555	0.006981	0.712102
-37.757853	-2.048746	1.626560	0.007028	0.712094
-37.908559	-2.019932	1.631565	0.007055	0.712098
-37.584740	-2.077496	1.636570	0.006994	0.712100
-37.910378	-2.025348	1.641574	0.007055	0.712089
-38.007724	-2.152841	1.646579	0.007072	0.711801
-38.791878	-2.031018	1.651584	0.007218	0.711766
-39.016619	-1.989406	1.656589	0.007259	0.711770
-38.723495	-2.042951	1.661594	0.007204	0.711769
-38.836777	-2.027262	1.666598	0.007225	0.711760
-38.877178	-2.014225	1.671603	0.007232	0.711773
-38.974746	-2.003450	1.676608	0.007249	0.711761
-38.721235	-2.143890	1.681613	0.007202	0.711572
-39.628175	-2.039264	1.686618	0.007370	0.711459
-39.945333	-1.983065	1.691622	0.007429	0.711459
-39.355930	-2.086971	1.696627	0.007318	0.711462
-39.666412	-2.035795	1.701632	0.007376	0.711455
-39.504370	-2.062036	1.706637	0.007345	0.711461
-39.671703	-2.031708	1.711642	0.007376	0.711463
-40.004816	-2.083119	1.716646	0.007437	0.711243
-40.555651	-2.033931	1.721651	0.007539	0.711146
-40.482600	-2.052100	1.726656	0.007525	0.711137
-40.517859	-2.043035	1.731661	0.007531	0.711143
-40.637261	-2.022615	1.736666	0.007553	0.711143
-40.726939	-2.010306	1.741670	0.007569	0.711136
-40.145595	-2.109455	1.746675	0.007461	0.711146
-40.571026	-2.121969	1.751680	0.007539	0.710971
-41.585535	-1.991672	1.756685	0.007728	0.710871
-41.277341	-2.045051	1.761690	0.007670	0.710875
-40.779843	-2.134542	1.766694	0.007577	0.710874
-40.838013	-2.122686	1.771699	0.007587	0.710878
-41.294493	-2.046118	1.776704	0.007672	0.710869
-41.394283	-2.037595	1.781709	0.007690	0.710852
-41.532445	-2.169232	1.786714	0.007715	0.710541
-42.283832	-2.038592	1.791718	0.007854	0.710535
-42.366931	-2.021592	1.796723	0.007869	0.710540
-42.063296	-2.081583	1.801728	0.007812	0.710529
-42.070089	-2.077553	1.806733	0.007813	0.710536
-42.196380	-2.053873	1.811738	0.007836	0.710539
-42.144112	-2.106071	1.816742	0.007826	0.710455
-42.979538	-2.072267	1.821747	0.007981	0.710226
-43.208324	-2.036260	1.826752	0.008023	0.710217
-43.244295	-2.027736	1.831757	0.008029	0.710222
-42.994285	-2.072588	1.836762	0.007982	0.710222
-43.217815	-2.035565	1.841766	0.008024	0.710218
-43.114051	-2.050377	1.846771	0.008004	0.710226
-43.011089	-2.080195	1.851776	0.007984	0.710204
-43.874728	-2.080194	1.856781	0.008144	0.709897
-44.085228	-2.043930	1.861786	0.008183	0.709896
-44.009204	-2.060709	1.866790	0.008168	0.709890
-43.673993	-2.116059	1.871795	0.008106	0.709900
-44.125819	-2.037654	1.876800	0.008189	0.709897
-44.386448	-1.989805	1.881805	0.008237	0.709900
-43.812722	-2.092493	1.886810	0.008130	0.709900
-44.469976	-2.096306	1.891814	0.008252	0.709659
-45.011013	-2.027674	1.896819	0.008352	0.709605
-44.824710	-2.065194	1.901824	0.008317	0.709597
-44.805527	-2.066266	1.906829	0.008313	0.709603
-45.061464	-2.020851	1.911834	0.008360	0.709603
-45.198715	-1.998067	1.916838	0.008385	0.709601
-44.922751	-2.045205	1.921843	0.008333	0.709606
-45.231951	-2.058134	1.926848	0.008390	0.709471
-46.169337	-1.991011	1.931853	0.008564	0.709272
-45.520763	-2.106846	1.936858	0.008443	0.709272
-45.990428	-2.024205	1.941862	0.008530	0.709271
-45.781604	-2.060201	1.946867	0.008491	0.709274
-45.571352	-2.101714	1.951872	0.008451	0.709267
-46.029624	-2.019037	1.956877	0.008536	0.709270
-46.146844	-2.014091	1.961882	0.008557	0.709239
-46.612013	-2.071885	1.966886	0.008643	0.708958
-46.440550	-2.097639	1.971891	0.008611	0.708969
-47.076039	-1.990358	1.976896	0.008729	0.708958
-46.793531	-2.038627	1.981901	0.008676	0.708963
-46.467500	-2.097536	1.986906	0.008615	0.708962
-47.024184	-2.000868	1.991910	0.008718	0.708958
-47.048587	-1.992538	1.996915	0.008722	0.708967
-47.445734	-2.062246	2.001920	0.008795	0.708686

-47.502791	-2.074924	2.011917	0.008805	0.708642
-47.719988	-2.035661	2.021914	0.008844	0.708645
-47.812533	-2.020289	2.031910	0.008861	0.708645
-47.851448	-2.013029	2.041907	0.008867	0.708648
-47.553236	-2.068068	2.051904	0.008811	0.708646
-47.919447	-2.003422	2.061901	0.008878	0.708646
-47.780045	-2.026885	2.071898	0.008851	0.708651
-48.094457	-1.971821	2.081894	0.008908	0.708651
-47.893885	-2.010279	2.091891	0.008870	0.708647
-47.912700	-2.008747	2.101888	0.008873	0.708645
-47.296216	-1.972205	2.111885	0.008757	0.708940
-46.921175	-2.027743	2.121882	0.008686	0.708965
-46.822374	-2.046545	2.131878	0.008667	0.708964
-47.004348	-2.015667	2.141875	0.008700	0.708963
-46.939224	-2.029170	2.151872	0.008687	0.708961
-47.103358	-1.977431	2.161869	0.008716	0.709008
-46.138796	-2.014232	2.171866	0.008536	0.709280
-45.984447	-2.044572	2.181862	0.008506	0.709276
-46.060925	-2.030150	2.191859	0.008519	0.709280
-46.145215	-2.017264	2.201856	0.008534	0.709278
-45.717653	-1.972968	2.211853	0.008453	0.709520
-45.479076	-1.969024	2.221850	0.008408	0.709615
-45.510573	-1.963827	2.231846	0.008413	0.709616
-45.472644	-1.957915	2.241843	0.008405	0.709643
-44.679083	-1.965909	2.251840	0.008256	0.709912
-44.590030	-1.982622	2.261837	0.008238	0.709912
-44.547920	-1.992611	2.271834	0.008230	0.709909
-44.310570	-1.953907	2.281830	0.008184	0.710073
-43.363484	-2.043320	2.291827	0.008007	0.710233
-43.602316	-2.004896	2.301824	0.008051	0.710227
-43.659348	-1.995501	2.311821	0.008060	0.710227
-42.968205	-2.003781	2.321818	0.007931	0.710459
-42.801774	-1.990043	2.331814	0.007899	0.710547
-42.612413	-2.022905	2.341811	0.007863	0.710551
-43.005472	-1.922738	2.351808	0.007935	0.710613
-41.871503	-1.992589	2.361805	0.007723	0.710879
-41.555921	-2.048878	2.371802	0.007663	0.710881
-41.990827	-1.971102	2.381798	0.007743	0.710883
-41.203669	-2.043973	2.391795	0.007595	0.711019
-41.254285	-1.972499	2.401792	0.007604	0.711146
-40.957764	-2.026056	2.411789	0.007548	0.711146
-40.960486	-2.017685	2.421786	0.007547	0.711164
-40.296981	-1.983077	2.431782	0.007423	0.711471
-40.173499	-2.009016	2.441779	0.007399	0.711465
-40.011850	-2.039326	2.451776	0.007368	0.711463
-39.870721	-1.985283	2.461773	0.007340	0.711623
-39.177825	-2.036615	2.471770	0.007210	0.711769
-39.438171	-1.989824	2.481766	0.007258	0.711772
-39.147231	-2.025377	2.491763	0.007203	0.711806
-38.630771	-1.971870	2.501760	0.007106	0.712098
-38.349207	-2.024209	2.511757	0.007052	0.712095
-38.233915	-2.045632	2.521754	0.007030	0.712095
-37.877117	-2.025151	2.531750	0.006963	0.712265
-37.693818	-1.992332	2.541747	0.006927	0.712397
-37.605637	-2.009395	2.551744	0.006910	0.712396
-37.500268	-2.007831	2.561741	0.006889	0.712439
-36.607396	-2.026851	2.571738	0.006722	0.712719
-36.637697	-2.021395	2.581734	0.006727	0.712721
-36.713973	-2.009436	2.591731	0.006740	0.712720
-36.237812	-1.988078	2.601728	0.006650	0.712933
-35.633365	-2.048353	2.611725	0.006537	0.713029
-35.851443	-2.006188	2.621722	0.006577	0.713038
-35.840066	-1.965439	2.631718	0.006574	0.713125
-34.866334	-2.014426	2.641715	0.006391	0.713374
-34.918568	-2.008676	2.651712	0.006400	0.713369
-34.988267	-1.998205	2.661709	0.006412	0.713367
-34.387104	-1.991582	2.671706	0.006299	0.713595
-34.083792	-2.011327	2.681702	0.006242	0.713665
-33.973388	-2.033057	2.691699	0.006220	0.713663
-34.251224	-1.934619	2.701696	0.006271	0.713762
-33.269675	-2.001660	2.711693	0.006087	0.713978
-33.146739	-2.027312	2.721690	0.006063	0.713973
-33.293147	-2.000859	2.731686	0.006090	0.713975
-32.312154	-2.025800	2.741683	0.005906	0.714275
-32.423272	-2.002486	2.751680	0.005926	0.714284
-31.990932	-2.081009	2.761677	0.005844	0.714282
-32.240273	-1.987524	2.771674	0.005890	0.714382
-31.250949	-2.048367	2.781670	0.005705	0.714613
-31.667795	-1.974569	2.791667	0.005781	0.714614
-31.520189	-2.002098	2.801664	0.005753	0.714613
-30.846176	-1.985518	2.811661	0.005626	0.714886
-30.622782	-2.011036	2.821658	0.005584	0.714916
-30.679442	-1.998520	2.831654	0.005593	0.714923
-30.230473	-1.990270	2.841651	0.005509	0.715100
-29.617398	-2.028122	2.851648	0.005394	0.715243
-29.848361	-1.986451	2.861645	0.005436	0.715246
-29.898726	-1.965602	2.871642	0.005444	0.715272
-28.809731	-2.012550	2.881638	0.005240	0.715565
-28.862976	-2.005763	2.891635	0.005249	0.715562
-28.863449	-2.007548	2.901632	0.005248	0.715560
-28.665389	-1.944786	2.911629	0.005211	0.715756
-27.663739	-2.055437	2.921626	0.005023	0.715892
-27.746843	-2.042032	2.931622	0.005038	0.715891
-27.954910	-2.005306	2.941619	0.005075	0.715892
-27.377832	-1.996000	2.951616	0.004967	0.716116
-27.198716	-2.018096	2.961613	0.004933	0.716138
-27.340407	-1.994296	2.971610	0.004958	0.716137
-26.681913	-2.009152	2.981606	0.004835	0.716341
-26.609534	-1.963154	2.991603	0.004820	0.716460
-26.251070	-2.029575	3.001600	0.004752	0.716456
-26.203256	-1.997818	3.011597	0.004743	0.716538
-25.280944	-2.051660	3.021594	0.004570	0.716758
-25.406847	-2.027989	3.031590	0.004592	0.716763
-25.503876	-2.012303	3.041587	0.004609	0.716761
-24.826357	-1.997593	3.051584	0.004482	0.717031
-24.571733	-2.014519	3.061581	0.004434	0.717089
-24.467222	-2.034567	3.071578	0.004413	0.717088
-24.372017	-1.999204	3.081574	0.004395	0.717194
-23.553760	-2.047557	3.091571	0.004241	0.717388
-23.743569	-2.014797	3.101568	0.004276	0.717388
-23.580543	-2.045621	3.111565	0.004245	0.717386
-22.944008	-2.039410	3.121562	0.004125	0.717624
-22.687465	-2.041590	3.131558	0.004076	0.717712
-22.742646	-2.032410	3.141555	0.004086	0.717713
-22.634555	-2.033132	3.151552	0.004065	0.717751
-21.930525	-2.022936	3.161549	0.003932	0.718021
-21.570098	-2.085274	3.171546	0.003864	0.718026
-21.681589	-2.065275	3.181542	0.003884	0.718029
-21.523292	-2.012038	3.191539	0.003854	0.718191
-20.899052	-2.037797	3.201536	0.003737	0.718362
-21.090614	-2.005201	3.211533	0.003771	0.718361
-20.847501	-2.047121	3.221530	0.003725	0.718365
-20.282197	-2.002871	3.231526	0.003619	0.718653
-19.849431	-2.080539	3.241523	0.003537	0.718654
-19.995796	-2.057299	3.251520	0.003564	0.718650
-20.050314	-1.977414	3.261517	0.003573	0.718790
-19.079316	-2.063966	3.271514	0.003391	0.718963
-19.254006	-2.032793	3.281510	0.003423	0.718965
-19.112138	-2.056799	3.291507	0.003395	0.718969
-18.474455	-2.015954	3.301504	0.003275	0.719275
-18.344434	-2.040068	3.311501	0.003250	0.719275
-18.111536	-2.082698	3.321498	0.003206	0.719275
-18.207244	-1.989430	3.331494	0.003223	0.719427
-17.286360	-2.061619	3.341491	0.003050	0.719610
-17.646768	-1.999598	3.351488	0.003116	0.719607
-17.355999	-2.049559	3.361485	0.003061	0.719613
-16.589564	-2.040212	3.371482	0.002918	0.719902
-16.657775	-2.028592	3.381478	0.002929	0.719903
-16.526795	-2.052599	3.391475	0.002904	0.719903
-16.103100	-2.036232	3.401472	0.002824	0.720086
-15.730281	-2.031968	3.411469	0.002754	0.720227
-15.594686	-2.057152	3.421466	0.002728	0.720227
-15.619818	-2.052132	3.431462	0.002731	0.720230
-14.803652	-2.043840	3.441459	0.002578	0.720534
-14.783648	-2.041219	3.451456	0.002574	0.720548
-14.768602	-2.046448	3.461453	0.002570	0.720545
-14.654569	-1.999156	3.471450	0.002548	0.720680
-13.795042	-2.046020	3.481446	0.002387	0.720890
-13.866306	-2.037829	3.491443	0.002399	0.720883
-14.016467	-2.012572	3.501440	0.002426	0.720882
-13.471737	-1.996563	3.511437	0.002324	0.721106
-13.224750	-2.029541	3.521434	0.002277	0.721130
-13.104019	-2.052872	3.531430	0.002253	0.721128
-12.874927	-1.985990	3.541427	0.002210	0.721342
-12.603799	-1.980934	3.551424	0.002158	0.721448
-12.345495	-2.029154	3.561421	0.002109	0.721446
-12.086638	-2.001512	3.571418	0.002060	0.721592
-11.509233	-2.019311	3.581414	0.001951	0.721761
-11.525130	-2.018000	3.591411	0.001953	0.721760
-11.662500	-1.967466	3.601408	0.001978	0.721813
-10.694652	-2.000725	3.611405	0.001797	0.722088
-10.567845	-2.026211	3.621402	0.001772	0.722084
-10.725073	-1.997353	3.631398	0.001801	0.722088
-10.180421	-1.975908	3.641395	0.001698	0.722322
-9.709433	-2.028838	3.651392	0.001610	0.722385
-9.804085	-2.015498	3.661389	0.001626	0.722380
-9.587276	-2.004149	3.671386	0.001585	0.722479
-8.805064	-2.024685	3.681382	0.001438	0.722714
-8.815264	-2.025543	3.691379	0.001439	0.722711
-8.962135	-2.000917	3.701376	0.001466	0.722710
-8.476402	-1.951744	3.711373	0.001374	0.722978
-8.202172	-1.976068	3.721370	0.001322	0.723028
-7.914575	-2.025238	3.731366	0.001268	0.723033
-7.701788	-1.980252	3.741363	0.001227	0.723198
-6.862905	-2.034858	3.751360	0.001070	0.723385
-6.961024	-2.019231	3.761357	0.001087	0.723383
-7.080678	-1.999691	3.771354	0.001109	0.723382
-6.857411	-1.922239	3.781350	0.001066	0.723613
-6.571932	-1.932710	3.791347	0.001012	0.723694
-6.203537	-1.997294	3.801344	0.000942	0.723698
-6.037794	-1.936433	3.811341	0.000910	0.723877
-5.471394	-1.957556	3.821338	0.000804	0.724035
-5.206688	-2.003203	3.831334	0.000754	0.724039
-5.252143	-1.996114	3.841331	0.000761	0.724039
-4.886271	-1.910446	3.851328	0.000692	0.724336
-4.551624	-1.964628	3.861325	0.000629	0.724349
-4.378967	-1.993529	3.871322	0.000596	0.724354
-4.140481	-1.959779	3.881318	0.000550	0.724505
-3.594927	-1.968848	3.891315	0.000448	0.724679
-3.674903	-1.958091	3.901312	0.000462	0.724674
-3.543262	-1.983522	3.911309	0.000436	0.724672
-3.203777	-1.902804	3.921306	0.000372	0.724950
-3.041337	-1.920534	3.931302	0.000341	0.724974
-3.048019	-1.920107	3.941299	0.000341	0.724974
-2.794947	-1.839572	3.951296	0.000293	0.725222
-2.420611	-1.873869	3.961293	0.000222	0.725287
-2.341832	-1.888533	3.971290	0.000207	0.725287
-2.071274	-1.803615	3.981286	0.000155	0.725549
-1.843122	-1.816116	3.991283	0.000112	0.725606
-1.707126	-1.843642	4.001280	0.000086	0.725601
-1.687813	-1.680546	4.011277	0.000081	0.725928
-1.625764	-1.690792	4.021274	0.000069	0.725932
-1.394686	-1.662707	4.031270	0.000025	0.726069
-1.355874	-1.599350	4.041267	0.000016	0.726208
-1.131289	-1.599501	4.051264	-0.000027	0.726287
-1.001973	-1.506310	4.061261	-0.000052	0.726516
-0.920957	-1.496387	4.071258	-0.000068	0.726565
-0.849438	-1.377524	4.081254	-0.000082	0.726824
-0.783135	-1.348869	4.091251	-0.000095	0.726905
-0.667791	-1.244435	4.101248	-0.000118	0.727150
-0.504517	-1.209211	4.111245	-0.000149	0.727277
-0.503173	-1.121307	4.121242	-0.000151	0.727451
-0.608892	-0.979964	4.131238	-0.000132	0.727692
-0.496473	-0.923448	4.141235	-0.000154	0.727843
-0.374672	-0.822084	4.151232	-0.000178	0.728084
-0.372862	-0.696196	4.161229	-0.000179	0.728332
-0.306180	-0.610877	4.171226	-0.000192	0.728523
-0.124480	-0.538929	4.181222	-0.000227	0.728727
-0.112792	-0.383430	4.191219	-0.000230	0.729036
-0.019844	-0.286774	4.201216	-0.000249	0.729258
-0.011665	-0.162175	4.211213	-0.000251	0.729505
-0.043883	-0.027329	4.221210	-0.000246	0.729757
0.019377	0.098620	4.231206	-0.000259	0.730026
0.000000	0.291464	4.241203	-0.000257	0.730395

0.222455	0.874754	4.246208	-0.000299	0.731604
0.300498	2.136304	4.251213	-0.000315	0.734073
0.506563	3.973293	4.256218	-0.000355	0.737685
0.714924	6.358273	4.261222	-0.000396	0.742327
1.108003	9.241997	4.266227	-0.000471	0.747949
1.395685	12.634170	4.271232	-0.000528	0.754450
1.927156	16.405258	4.276237	-0.000629	0.761682
2.413450	20.620887	4.281242	-0.000723	0.769650
2.784687	25.245805	4.286246	-0.000796	0.778245
3.344563	30.212439	4.291251	-0.000904	0.787422
3.922562	35.517955	4.296256	-0.001015	0.797102
4.272627	41.178701	4.301261	-0.001085	0.807218
4.862969	47.115733	4.306266	-0.001199	0.817763
5.260720	53.356861	4.311270	-0.001278	0.828634
5.977227	59.818761	4.316275	-0.001416	0.839833
6.289655	66.565680	4.321280	-0.001479	0.851240
6.674978	73.514270	4.326285	-0.001556	0.862849
7.375579	80.628183	4.331290	-0.001691	0.874661
7.733149	87.964937	4.336294	-0.001763	0.886576
8.205027	95.468545	4.341299	-0.001856	0.898627
8.758867	103.113442	4.346304	-0.001965	0.910760
10.561650	110.662090	4.351309	-0.002306	0.922923
15.767874	117.820788	4.356314	-0.003280	0.935237
16.204476	125.950486	4.361318	-0.003367	0.947594
16.802773	134.160070	4.366323	-0.003485	0.959951
17.366844	142.444790	4.371328	-0.003596	0.972252
18.064577	150.787085	4.376333	-0.003731	0.984515
19.010607	159.187526	4.381338	-0.003914	0.996771
19.910336	167.592609	4.386342	-0.004087	1.008872
20.775538	176.072653	4.391347	-0.004254	1.020926
21.371929	184.633122	4.396352	-0.004371	1.032884
22.295273	193.156563	4.401357	-0.004549	1.044732
23.213819	201.728964	4.406362	-0.004726	1.056511
24.056453	210.317887	4.411366	-0.004889	1.068165
25.083247	218.915633	4.416371	-0.005087	1.079745
25.538405	227.607416	4.421376	-0.005177	1.091196
26.213537	236.253278	4.426381	-0.005309	1.102517
27.003687	244.917979	4.431386	-0.005463	1.113772
27.584562	253.570795	4.436390	-0.005577	1.124854
28.138573	262.261711	4.441395	-0.005686	1.135869
28.792928	270.906105	4.446400	-0.005814	1.146742
29.627320	279.547514	4.451405	-0.005976	1.157546
30.098450	288.205274	4.456410	-0.006069	1.168195
30.475587	296.853664	4.461414	-0.006146	1.178716
31.275588	305.437632	4.466419	-0.006301	1.189154
31.970886	314.023685	4.471424	-0.006436	1.199481
32.786816	322.580253	4.476429	-0.006594	1.209709
33.600830	331.139643	4.481434	-0.006752	1.219855
34.117345	339.732966	4.486438	-0.006854	1.229897
34.951919	348.261401	4.491443	-0.007016	1.239845
35.432170	356.816904	4.496448	-0.007111	1.249676
36.029412	365.340942	4.501453	-0.007228	1.259417
36.894956	373.826201	4.506458	-0.007396	1.269090
37.416922	382.341369	4.511462	-0.007499	1.278658
38.143199	390.810865	4.516467	-0.007640	1.288143
38.790206	399.296019	4.521472	-0.007767	1.297560
39.385470	407.770519	4.526477	-0.007883	1.306889
40.032854	416.361499	4.531482	-0.008010	1.316286
40.709266	424.741915	4.536486	-0.008142	1.325396
41.387550	433.156194	4.541491	-0.008274	1.334480
41.990644	441.555780	4.546496	-0.008392	1.343473
42.999452	449.897656	4.551501	-0.008586	1.352417
43.440921	458.317895	4.556506	-0.008674	1.361285
43.975567	466.719152	4.561510	-0.008780	1.370091
44.823868	475.069019	4.566515	-0.008944	1.378842
45.328240	483.466634	4.571520	-0.009044	1.387528
45.863412	491.855848	4.576525	-0.009149	1.396156
46.580120	500.183113	4.581530	-0.009289	1.404698
47.156609	508.538050	4.586534	-0.009402	1.413194
47.590892	516.891373	4.591539	-0.009489	1.421613
47.963021	525.251758	4.596544	-0.009564	1.429979
48.503261	533.570464	4.601549	-0.009670	1.438283
49.197741	541.850210	4.606554	-0.009806	1.446526
49.646202	550.183701	4.611558	-0.009895	1.454734
50.268185	558.476662	4.616563	-0.010017	1.462885
50.847861	566.798601	4.621568	-0.010130	1.471011
51.207061	575.132927	4.626573	-0.010203	1.479070
51.826273	583.390433	4.631578	-0.010324	1.487052
52.517173	591.637819	4.636582	-0.010459	1.494993
52.752656	599.961409	4.641587	-0.010509	1.502894
53.072657	608.256462	4.646592	-0.010574	1.510739
53.913379	616.459001	4.651597	-0.010737	1.518537
54.558469	624.690184	4.656602	-0.010863	1.526291
54.949852	632.972477	4.661606	-0.010941	1.534015
55.289860	641.247277	4.666611	-0.011010	1.541685
55.953065	649.478829	4.671616	-0.011140	1.549326
56.462626	657.732112	4.676621	-0.011241	1.556926
56.836401	665.981763	4.681626	-0.011316	1.564466
57.436607	674.199679	4.686630	-0.011434	1.571974
58.179792	682.398582	4.691635	-0.011578	1.579450
58.568221	690.647109	4.696640	-0.011656	1.586883
59.042746	698.882328	4.701645	-0.011750	1.594283
59.471251	707.112772	4.706650	-0.011836	1.601637
59.683079	715.355129	4.711654	-0.011881	1.608937
60.275936	723.562110	4.716659	-0.011997	1.616226
60.701457	731.771159	4.721664	-0.012082	1.623461
60.783937	740.051107	4.726669	-0.012104	1.630678
61.688534	748.222689	4.731674	-0.012278	1.637883
62.345020	756.345500	4.736678	-0.012406	1.644980
62.848509	764.553820	4.741683	-0.012505	1.652098
63.128964	772.779431	4.746688	-0.012564	1.659170
63.785115	780.915478	4.751693	-0.012692	1.666187
64.624036	789.086212	4.756698	-0.012854	1.673228
64.903726	797.290783	4.761702	-0.012911	1.680193
65.252996	805.492518	4.766707	-0.012982	1.687136
65.948892	813.659725	4.771712	-0.013118	1.694067
66.290180	821.845986	4.776717	-0.013187	1.700940
66.806200	830.038808	4.781722	-0.013289	1.707812
67.052513	838.264334	4.786726	-0.013341	1.714649
67.580914	846.404271	4.791731	-0.013445	1.721425
68.010133	854.561359	4.796736	-0.013531	1.728175
68.482051	862.740496	4.801741	-0.013624	1.734922
68.920986	870.900883	4.806746	-0.013712	1.741624
69.485617	879.046937	4.811750	-0.013823	1.748304
70.108398	887.211034	4.816755	-0.013944	1.754980
70.512954	895.373289	4.821760	-0.014026	1.761602
70.939822	903.530464	4.826765	-0.014111	1.768198
71.113679	911.757108	4.831770	-0.014149	1.774793
71.358629	919.917085	4.836774	-0.014200	1.781319
71.987156	928.048772	4.841779	-0.014323	1.787846
72.359996	936.269814	4.846784	-0.014399	1.794389
72.805208	944.375008	4.851789	-0.014487	1.800825
73.712912	952.439020	4.856794	-0.014662	1.807262
74.243121	960.580714	4.861798	-0.014766	1.813691
74.741503	968.713980	4.866803	-0.014865	1.820087
75.078376	976.875828	4.871808	-0.014934	1.826463
75.668689	985.005165	4.876813	-0.015049	1.832822
76.245153	993.138871	4.881818	-0.015162	1.839160
76.640631	1001.269100	4.886822	-0.015242	1.845452
77.105498	1009.436055	4.891827	-0.015334	1.851759
77.803052	1017.554555	4.896832	-0.015470	1.858035
78.326658	1025.672413	4.901837	-0.015573	1.864269
78.835156	1033.838001	4.906842	-0.015674	1.870516
78.946156	1042.021727	4.911846	-0.015700	1.876710
79.312543	1050.153494	4.916851	-0.015774	1.882874
79.775002	1058.267464	4.921856	-0.015866	1.889015
80.259320	1066.393679	4.926861	-0.015962	1.895148
80.724462	1074.506378	4.931866	-0.016054	1.901249
80.827118	1082.669689	4.936870	-0.016079	1.907327
81.414746	1090.785474	4.941875	-0.016194	1.913404
81.713017	1098.913457	4.946880	-0.016256	1.919439
81.851535	1107.055057	4.951885	-0.016287	1.925448
82.502109	1115.158612	4.956890	-0.016414	1.931466
82.842234	1123.285739	4.961894	-0.016483	1.937448
83.504302	1131.364908	4.966899	-0.016612	1.943412
84.088942	1139.473785	4.971904	-0.016727	1.949371
84.466573	1147.639633	4.976909	-0.016803	1.955330
84.892996	1155.742526	4.981914	-0.016888	1.961231
85.054624	1163.868284	4.986918	-0.016924	1.967102
85.211285	1172.032065	4.991923	-0.016959	1.972983
85.975225	1180.058996	4.996928	-0.017107	1.978812
86.279173	1188.159383	5.001933	-0.017169	1.984628
87.072222	1196.237982	5.006938	-0.017323	1.990463
87.516859	1204.348363	5.011942	-0.017411	1.996266
87.757402	1212.479826	5.016947	-0.017462	2.002046
87.908952	1220.620260	5.021952	-0.017496	2.007807
88.530249	1228.693741	5.026957	-0.017617	2.013552
89.031829	1236.804016	5.031962	-0.017717	2.019295
89.498845	1244.875424	5.036966	-0.017809	2.024990
90.036351	1252.990511	5.041971	-0.017915	2.030707
90.424634	1261.131521	5.046976	-0.017993	2.036410
90.639361	1269.240031	5.051981	-0.018039	2.042058
90.996617	1277.345559	5.056986	-0.018111	2.047702
91.229183	1285.462317	5.061990	-0.018160	2.053325
91.581761	1293.560827	5.066995	-0.018232	2.058933
92.099364	1301.625293	5.072000	-0.018334	2.064518
92.561063	1309.715149	5.077005	-0.018426	2.070100
93.108803	1317.825704	5.082010	-0.018533	2.075690
93.254111	1325.921044	5.087014	-0.018566	2.081214
93.790263	1333.989147	5.092019	-0.018672	2.086743
94.318934	1342.102571	5.097024	-0.018776	2.092288
94.830032	1350.184008	5.102029	-0.018877	2.097795
95.339335	1358.284571	5.107034	-0.018977	2.103299
95.493977	1366.404190	5.112038	-0.019012	2.108768
95.807190	1374.604541	5.117043	-0.019076	2.114292
96.111463	1382.671850	5.122048	-0.019139	2.119711
96.404770	1390.728331	5.127053	-0.019199	2.125109
96.798291	1398.821016	5.132058	-0.019278	2.130526
97.013140	1406.917085	5.137062	-0.019324	2.135915
97.447546	1414.979201	5.142067	-0.019410	2.141288
98.026272	1423.027786	5.147072	-0.019524	2.146653
98.010191	1431.185172	5.152077	-0.019527	2.152020
98.220578	1439.291365	5.157082	-0.019572	2.157361
98.916805	1447.268479	5.162086	-0.019707	2.162649
99.253087	1455.374954	5.167091	-0.019775	2.167976
99.283518	1463.506902	5.172096	-0.019787	2.173277
99.681143	1471.561023	5.177101	-0.019866	2.178549
100.219911	1479.626559	5.182106	-0.019973	2.183829
100.561260	1487.707068	5.187110	-0.020042	2.189087
101.109426	1495.811997	5.192115	-0.020150	2.194367
101.663659	1503.856380	5.197120	-0.020259	2.199596
101.867194	1511.940234	5.202125	-0.020302	2.204806
102.422772	1520.023418	5.207130	-0.020411	2.210035
102.546548	1528.140306	5.212134	-0.020440	2.215234
102.827754	1536.237642	5.217139	-0.020498	2.220423
103.392260	1544.266098	5.222144	-0.020609	2.225580
103.690928	1552.374142	5.227149	-0.020671	2.230753
104.041231	1560.464168	5.232154	-0.020742	2.235907
104.153957	1568.534494	5.237158	-0.020768	2.241015
104.498743	1576.598974	5.242163	-0.020838	2.246129
104.740559	1584.707335	5.247168	-0.020889	2.251249
105.211257	1592.767219	5.252173	-0.020982	2.256348
105.640865	1600.826661	5.257178	-0.021068	2.261430
106.060861	1608.885118	5.262182	-0.021152	2.266500
106.377094	1617.023410	5.267187	-0.021217	2.271599
106.800643	1625.121943	5.272192	-0.021301	2.276672
107.257428	1633.141073	5.277197	-0.021392	2.281686
107.816660	1641.179484	5.282202	-0.021502	2.286710
107.965531	1649.274889	5.287206	-0.021535	2.291723
108.274849	1657.356750	5.292211	-0.021599	2.296730
108.515796	1665.443990	5.297216	-0.021649	2.301724
108.905946	1673.489352	5.302221	-0.021728	2.306694
109.140603	1681.588642	5.307226	-0.021777	2.311673
109.395701	1689.659815	5.312230	-0.021831	2.316626
109.817084	1697.700176	5.317235	-0.021915	2.321564
109.999291	1705.780976	5.322240	-0.021954	2.326495
110.461959	1713.829653	5.327245	-0.022046	2.331420
110.941520	1721.898289	5.332250	-0.022141	2.336347
111.257392	1729.952696	5.337254	-0.022206	2.341243
111.512066	1738.032721	5.342259	-0.022259	2.346138
111.687402	1746.153237	5.347264	-0.022297	2.351041
112.229076	1754.196717	5.352269	-0.022404	2.355917
112.579749	1762.251931	5.357274	-0.022475	2.360774
112.866258	1770.301003	5.362278	-0.022534	2.365613
113.282718	1778.362932	5.367283	-0.022617	2.370460
113.610609	1786.464013	5.372288	-0.022684	2.375313
113.748910	1794.517908	5.377293	-0.022716	2.380113
114.284701	1802.576931	5.382298	-0.022821	2.384937
114.584854	1810.627346	5.387302	-0.022883	2.389729
114.821010	1818.740201	5.392307	-0.022933	2.394542
115.161258	1826.791060	5.397312	-0.023002	2.399317
115.478961	1834.831193	5.402317	-0.023067	2.404075
115.778136	1842.910679	5.407322	-0.023128	2.408845
115.855678	1851.014683	5.412326	-0.023148	2.413602
116.273009	1859.056165	5.417331	-0.023232	2.418340
116.415365	1867.134220	5.422336	-0.023264	2.423068
116.779659	1875.171289	5.427341	-0.023337	2.427781
117.142496	1883.288077	5.432346	-0.023411	2.432530
117.278299	1891.367117	5.437350	-0.023442	2.437231
117.725175	1899.373032	5.442355	-0.023531	2.441905
118.035934	1907.421067	5.447360	-0.023594	2.446583
118.300423	1915.485088	5.452365	-0.023649	2.451258
118.501152	1923.573558	5.457370	-0.023692	2.455933
118.850896	1931.594832	5.462374	-0.023763	2.460572
119.366055	1939.624091	5.467379	-0.023865	2.465219
119.612436	1947.708433	5.472384	-0.023917	2.469868
119.942050	1955.762393	5.477389	-0.023984	2.474498
120.500662	1963.805801	5.482394	-0.024093	2.479130
120.805812	1971.854366	5.487398	-0.024156	2.483737
121.033374	1979.930036	5.492403	-0.024204	2.488345
121.318871	1988.013630	5.497408	-0.024263	2.492954
121.589549	1996.057464	5.502413	-0.024319	2.497530
122.082492	2004.105322	5.507418	-0.024417	2.502117
122.424957	2012.147735	5.512422	-0.024486	2.506681
122.824955	2020.227330	5.517427	-0.024566	2.511261
123.316696	2028.300743	5.522432	-0.024664	2.515836
123.426130	2036.353438	5.527437	-0.024690	2.520364
123.924383	2044.373838	5.532442	-0.024788	2.524894
124.007416	2052.451000	5.537446	-0.024809	2.529417
124.339855	2060.521293	5.542451	-0.024877	2.533946
124.844522	2068.546506	5.547456	-0.024977	2.538454
125.058350	2076.590070	5.552461	-0.025022	2.542944
125.201375	2084.694103	5.557466	-0.025055	2.547454
125.365148	2092.753601	5.562470	-0.025091	2.551933
125.805926	2100.795208	5.567475	-0.025179	2.556413
126.054447	2108.859327	5.572480	-0.025231	2.560885
126.174809	2116.903686	5.577485	-0.025259	2.565329
126.678694	2124.946795	5.582490	-0.025358	2.569791
127.021330	2133.003968	5.587494	-0.025428	2.574242
127.163820	2141.069910	5.592499	-0.025460	2.578676
127.446363	2149.114621	5.597504	-0.025519	2.583101
127.681572	2157.168358	5.602509	-0.025568	2.587519
128.460425	2165.270143	5.607514	-0.025719	2.591993
128.636169	2173.434840	5.612518	-0.025757	2.596453
128.779055	2181.432468	5.617523	-0.025790	2.600812
129.065974	2189.431774	5.622528	-0.025849	2.605174
129.095505	2197.465615	5.627533	-0.025860	2.609531
129.526757	2205.526728	5.632538	-0.025946	2.613921
129.780620	2213.539122	5.637542	-0.025999	2.618266
129.924759	2221.597932	5.642547	-0.026032	2.622622
130.169497	2229.642758	5.647552	-0.026083	2.626969
130.387062	2237.689002	5.652557	-0.026129	2.631308
130.839813	2245.749207	5.657562	-0.026219	2.635663
130.973692	2253.764109	5.662566	-0.026250	2.639966
131.545841	2261.756956	5.667571	-0.026362	2.644278
131.855805	2269.826536	5.672576	-0.026425	2.648607
131.769818	2277.930253	5.677581	-0.026415	2.652921
132.468949	2285.949763	5.682586	-0.026551	2.657234
132.452338	2294.037981	5.687590	-0.026554	2.661531
132.640161	2302.078527	5.692595	-0.026594	2.665808
133.068085	2310.121304	5.697600	-0.026680	2.670096
133.407624	2318.202735	5.702605	-0.026749	2.674390
133.891508	2326.196481	5.707610	-0.026845	2.678641
134.151784	2334.225437	5.712614	-0.026899	2.682890
134.204685	2342.285122	5.717619	-0.026914	2.687135
134.683749	2350.331350	5.722624	-0.027009	2.691392
134.926137	2358.388631	5.727629	-0.027060	2.695634
135.384905	2366.410165	5.732634	-0.027151	2.699864
135.629160	2374.465429	5.737638	-0.027203	2.704092
135.920544	2382.517651	5.742643	-0.027263	2.708314
136.046247	2390.615553	5.747648	-0.027292	2.712543
136.151192	2398.637395	5.752653	-0.027317	2.716725
136.607468	2406.667205	5.757658	-0.027408	2.720926
136.742809	2414.687544	5.762662	-0.027439	2.725095
137.169581	2422.744852	5.767667	-0.027524	2.729296
137.466932	2430.817443	5.772672	-0.027585	2.733489
137.509540	2438.876413	5.777677	-0.027599	2.737654
138.023649	2446.906074	5.782682	-0.027700	2.741826
138.303592	2454.941222	5.787686	-0.027758	2.745980
138.418512	2463.009909	5.792691	-0.027785	2.750135
138.362533	2471.200384	5.797696	-0.027780	2.754336
138.803516	2479.149500	5.802701	-0.027868	2.758437
139.169710	2487.160345	5.807706	-0.027942	2.762559
139.140156	2495.203851	5.812710	-0.027942	2.766667
139.332852	2503.248123	5.817715	-0.027984	2.770783
139.713200	2511.279596	5.822720	-0.028060	2.774898
139.863171	2519.303886	5.827725	-0.028094	2.778989
140.395316	2527.322884	5.832730	-0.028199	2.783094
140.465399	2535.372359	5.837734	-0.028218	2.787181
140.951443	2543.415283	5.842739	-0.028314	2.791283
141.042144	2551.498591	5.847744	-0.028336	2.795376
141.364265	2559.504072	5.852749	-0.028402	2.799437
141.714821	2567.544125	5.857754	-0.028473	2.803512
141.730163	2575.589844	5.862758	-0.028482	2.807564
142.126956	2583.627151	5.867763	-0.028561	2.811628
142.665025	2591.682579	5.872768	-0.028667	2.815703
142.769768	2599.709676	5.877773	-0.028692	2.819733
142.880805	2607.787552	5.882778	-0.028719	2.823783
143.169411	2615.817534	5.887782	-0.028778	2.827814
143.376657	2623.911563	5.892787	-0.028823	2.831866
143.570505	2631.978713	5.897792	-0.028864	2.835898
144.004719	2639.945539	5.902797	-0.028951	2.839888
144.493540	2647.962282	5.907802	-0.029048	2.843900
144.725740	2656.003809	5.912806	-0.029097	2.847904
144.867358	2664.060678	5.917811	-0.029129	2.851905
145.132339	2672.145396	5.922816	-0.029184	2.855922
145.525688	2680.129909	5.927821	-0.029263	2.859890
145.921808	2688.164674	5.932826	-0.029342	2.863877
145.993644	2696.214761	5.937830	-0.029361	2.867849
146.421705	2704.274418	5.942835	-0.029447	2.871839
146.613999	2712.343805	5.947840	-0.029488	2.875815
146.807577	2720.338397	5.952845	-0.029530	2.879750
147.156634	2728.372685	5.957850	-0.029601	2.883706
147.386193	2736.401438	5.962854	-0.029649	2.887649
147.699410	2744.443556	5.967859	-0.029713	2.891596
148.049196	2752.520333	5.972864	-0.029784	2.895558
148.088342	2760.538749	5.977869	-0.029797	2.899468
148.392437	2768.597297	5.982874	-0.029860	2.903407
148.513594	2776.627912	5.987878	-0.029888	2.907318
149.039205	2784.679809	5.992883	-0.029991	2.911254
149.156697	2792.810728	5.997888	-0.030019	2.915202
149.519919	2800.780081	6.002893	-0.030092	2.919080
149.622029	2808.822284	6.007898	-0.030117	2.922974
149.969623	2816.806519	6.012902	-0.030188	2.926847
150.131581	2824.849540	6.017907	-0.030223	2.930734
150.371286	2832.909830	6.022912	-0.030274	2.934628
150.405418	2840.938888	6.027917	-0.030286	2.938491
150.916289	2848.958288	6.032922	-0.030387	2.942369
150.984577	2857.011500	6.037926	-0.030405	2.946236
151.409152	2865.030485	6.042931	-0.030490	2.950099
151.895315	2873.073196	6.047936	-0.030586	2.953971
151.905862	2881.107739	6.052941	-0.030594	2.957811
152.214798	2889.133907	6.057946	-0.030657	2.961656
152.370863	2897.157501	6.062950	-0.030692	2.965487
152.545715	2905.228950	6.067955	-0.030730	2.969337
153.149418	2913.260090	6.072960	-0.030848	2.973185
153.494909	2921.257644	6.077965	-0.030918	2.976998
153.768749	2929.318712	6.082970	-0.030975	2.980833
153.970558	2937.349105	6.087974	-0.031018	2.984645
154.010263	2945.428804	6.092979	-0.031031	2.988468
154.611357	2953.453086	6.097984	-0.031149	2.992287
154.711926	2961.508811	6.102989	-0.031174	2.996091
155.070771	2969.508580	6.107994	-0.031246	2.999877
155.477727	2977.497669	6.112998	-0.031328	3.003655
155.783638	2985.538866	6.118003	-0.031390	3.007448
155.955718	2993.616342	6.123008	-0.031428	3.011246
156.187244	3001.651924	6.128013	-0.031477	3.015023
156.347016	3009.709181	6.133018	-0.031512	3.018802
156.385783	3017.739067	6.138022	-0.031525	3.022558
156.501824	3025.801741	6.143027	-0.031553	3.026328
156.799417	3033.827619	6.148032	-0.031614	3.030084
157.090064	3041.858300	6.153037	-0.031674	3.033838
157.539249	3049.889468	6.158042	-0.031763	3.037595
157.692733	3057.928283	6.163046	-0.031797	3.041337
157.961481	3065.920815	6.168051	-0.031853	3.045058
158.301436	3073.969233	6.173056	-0.031922	3.048804
158.516324	3082.002050	6.178061	-0.031968	3.052532
159.059544	3090.041709	6.183066	-0.032075	3.056274
159.220208	3098.057403	6.188070	-0.032110	3.059982
159.482888	3106.080669	6.193075	-0.032165	3.063694
159.713309	3114.159139	6.198080	-0.032214	3.067426
159.937754	3122.200640	6.203085	-0.032261	3.071135
160.210398	3130.322592	6.208090	-0.032318	3.074879
160.393343	3138.308424	6.213094	-0.032357	3.078552
160.548559	3146.312821	6.218099	-0.032392	3.082228
160.958324	3154.319026	6.223104	-0.032474	3.085912
161.489805	3162.310511	6.228109	-0.032579	3.089591
161.905618	3170.366475	6.233114	-0.032662	3.093289
161.993632	3178.416421	6.238118	-0.032684	3.096965
162.426898	3186.429907	6.243123	-0.032770	3.100635
162.708105	3194.466875	6.248128	-0.032828	3.104305
162.760862	3202.503889	6.253133	-0.032844	3.107960
162.928281	3210.592022	6.258138	-0.032881	3.111639
163.287935	3218.596401	6.263142	-0.032953	3.115285
163.710280	3226.612437	6.268147	-0.033038	3.118934
163.809813	3234.657456	6.273152	-0.033062	3.122578
163.862097	3242.698601	6.278157	-0.033078	3.126214
164.163643	3250.725375	6.283162	-0.033139	3.129850
164.259926	3258.770657	6.288166	-0.033163	3.133480
164.504842	3266.798313	6.293171	-0.033214	3.137106
164.975060	3274.815498	6.298176	-0.033308	3.140732
165.356632	3282.785452	6.303181	-0.033384	3.144329
165.828741	3290.868729	6.308186	-0.033478	3.147976
166.152573	3298.905602	6.313190	-0.033544	3.151592
166.327710	3306.981615	6.318195	-0.033582	3.155215
166.549285	3314.989863	6.323200	-0.033629	3.158805
166.718747	3323.003271	6.328205	-0.033667	3.162391
167.110865	3331.017764	6.333210	-0.033745	3.165984
167.268735	3339.045815	6.338214	-0.033780	3.169568
167.476520	3347.109142	6.343219	-0.033825	3.173165
167.781814	3355.184361	6.348224	-0.033887	3.176769
168.002651	3363.171447	6.353229	-0.033934	3.180325
168.434914	3371.209443	6.358234	-0.034020	3.183909
168.743617	3379.208528	6.363238	-0.034084	3.187466
168.924568	3387.247875	6.368243	-0.034123	3.191031
169.204080	3395.323736	6.373248	-0.034181	3.194613
169.484221	3403.324568	6.378253	-0.034239	3.198158
169.806075	3411.361656	6.383258	-0.034304	3.201716
169.909726	3419.378732	6.388262	-0.034329	3.205253
170.131571	3427.418480	6.393267	-0.034376	3.208801
170.481131	3435.473766	6.398272	-0.034447	3.212356
170.652210	3443.519260	6.403277	-0.034485	3.215896
170.834552	3451.516403	6.408282	-0.034524	3.219412
171.180894	3459.525670	6.413286	-0.034595	3.222935
171.509060	3467.555559	6.418291	-0.034661	3.226463
171.485649	3475.617679	6.423296	-0.034663	3.229987
171.587210	3483.715677	6.428301	-0.034687	3.233527
172.249153	3491.701475	6.433306	-0.034816	3.237038
172.391364	3499.697506	6.438310	-0.034849	3.240528
172.476340	3507.706055	6.443315	-0.034870	3.244017
172.845405	3515.742507	6.448320	-0.034945	3.247527
173.117744	3523.745623	6.453325	-0.035001	3.251013
173.314336	3531.821981	6.458330	-0.035043	3.254525
173.433222	3539.858024	6.463334	-0.035071	3.258013
173.622633	3547.897781	6.468339	-0.035112	3.261501
173.691756	3555.929703	6.473344	-0.035131	3.264978
173.801207	3563.944165	6.478349	-0.035157	3.268444
174.280251	3571.977271	6.483354	-0.035252	3.271930
174.486341	3580.027101	6.488358	-0.035296	3.275408
174.753308	3588.011940	6.493363	-0.035351	3.278857
175.219114	3596.036149	6.498368	-0.035444	3.282327
175.373381	3604.053341	6.503373	-0.035478	3.285778
175.629671	3612.120876	6.508378	-0.035532	3.289251
175.692320	3620.161141	6.513382	-0.035549	3.292701
175.982780	3628.207862	6.518387	-0.035609	3.296159
176.172520	3636.198383	6.523392	-0.035650	3.299585
176.306157	3644.219083	6.528397	-0.035680	3.303019
176.696744	3652.262825	6.533402	-0.035759	3.306468
176.824634	3660.267272	6.538406	-0.035788	3.309887
177.077227	3668.343145	6.543411	-0.035841	3.313338
177.428856	3676.383660	6.548416	-0.035912	3.316774
177.823047	3684.329797	6.553421	-0.035991	3.320167
178.013858	3692.388788	6.558426	-0.036033	3.323598
178.311856	3700.415218	6.563430	-0.036094	3.327015
178.765791	3708.391549	6.568435	-0.036184	3.330413
179.071626	3716.487939	6.573440	-0.036247	3.333853
179.195536	3724.510379	6.578445	-0.036276	3.337251
179.645246	3732.522551	6.583450	-0.036365	3.340653
179.730008	3740.532370	6.588454	-0.036386	3.344038
179.901462	3748.586602	6.593459	-0.036424	3.347441
179.995306	3756.651327	6.598464	-0.036447	3.350842
180.446313	3764.670744	6.603469	-0.036537	3.354233
180.732693	3772.711807	6.608474	-0.036596	3.357625
180.813107	3780.740007	6.613478	-0.036617	3.360999
181.078471	3788.718926	6.618483	-0.036672	3.364357
181.583473	3796.749729	6.623488	-0.036772	3.367741
181.672544	3804.808360	6.628493	-0.036794	3.371119
182.101901	3812.853143	6.633498	-0.036880	3.374499
182.422476	3820.862292	6.638502	-0.036945	3.377858
182.617261	3828.875168	6.643507	-0.036987	3.381210
182.722031	3836.905883	6.648512	-0.037012	3.384563
182.877712	3844.930620	6.653517	-0.037047	3.387912
183.124268	3852.983570	6.658522	-0.037099	3.391272
183.312654	3861.095294	6.663526	-0.037139	3.394652
183.560138	3869.081716	6.668531	-0.037191	3.397978
183.790865	3877.109841	6.673536	-0.037240	3.401318
183.909534	3885.046734	6.678541	-0.037268	3.404612
184.366371	3893.066086	6.683546	-0.037358	3.407949
184.628236	3901.108792	6.688550	-0.037413	3.411286
184.781428	3909.144989	6.693555	-0.037447	3.414613
185.202565	3917.154332	6.698560	-0.037531	3.417935
185.377094	3925.160753	6.703565	-0.037569	3.421244
185.473754	3933.203332	6.708570	-0.037593	3.424562
185.747933	3941.231006	6.713574	-0.037650	3.427877
186.036569	3949.293513	6.718579	-0.037709	3.431203
186.267862	3957.328337	6.723584	-0.037758	3.434513
186.476894	3965.297502	6.728589	-0.037803	3.437791
186.901423	3973.381948	6.733594	-0.037888	3.441121
187.165082	3981.357747	6.738598	-0.037942	3.444398
187.184149	3989.402048	6.743603	-0.037952	3.447692
187.430668	3997.454234	6.748608	-0.038003	3.450993
187.754945	4005.491244	6.753613	-0.038069	3.454287
188.057094	4013.517949	6.758618	-0.038131	3.457574
188.319912	4021.535642	6.763622	-0.038186	3.460852
188.566398	4029.518657	6.768627	-0.038238	3.464112
188.712095	4037.611654	6.773632	-0.038270	3.467411
189.033665	4045.617181	6.778637	-0.038336	3.470676
189.363362	4053.715115	6.783642	-0.038403	3.473977
189.631158	4061.668754	6.788646	-0.038459	3.477213
189.641769	4069.707784	6.793651	-0.038466	3.480473
190.012299	4077.684706	6.798656	-0.038541	3.483716
190.173011	4085.675503	6.803661	-0.038577	3.486955
190.344963	4093.748648	6.808666	-0.038614	3.490225
190.421002	4101.784282	6.813670	-0.038634	3.493474
190.961265	4109.830361	6.818675	-0.038741	3.496738
191.140283	4117.830646	6.823680	-0.038780	3.499969
191.351709	4125.830501	6.828685	-0.038825	3.503198
191.367968	4133.924950	6.833690	-0.038834	3.506456
191.644904	4141.898300	6.838694	-0.038891	3.509670
191.940178	4149.946904	6.843699	-0.038951	3.512913
191.982645	4158.016047	6.848704	-0.038965	3.516152
192.298697	4165.958997	6.853709	-0.039030	3.519347
192.585733	4173.988700	6.858714	-0.039089	3.522572
192.735367	4182.045615	6.863718	-0.039122	3.525801
192.983671	4190.055713	6.868723	-0.039174	3.529012
193.176989	4198.117223	6.873728	-0.039216	3.532238
193.191246	4206.147144	6.878733	-0.039224	3.535443
193.552086	4214.190659	6.883738	-0.039297	3.538661
193.902068	4222.215038	6.888742	-0.039368	3.541869
194.154680	4230.177172	6.893747	-0.039421	3.545045
194.426202	4238.267703	6.898752	-0.039477	3.548271
194.786988	4246.274244	6.903757	-0.039550	3.551462
195.068243	4254.398664	6.908762	-0.039608	3.554695
195.029763	4262.361101	6.913766	-0.039607	3.557852
195.320334	4270.353835	6.918771	-0.039667	3.561027
195.704959	4278.323314	6.923776	-0.039744	3.564193
196.000940	4286.327043	6.928781	-0.039805	3.567368
196.121096	4294.370560	6.933786	-0.039833	3.570550
196.537184	4302.407818	6.938790	-0.039916	3.573735
196.601772	4310.466718	6.943795	-0.039934	3.576915
196.898514	4318.455100	6.948800	-0.039995	3.580072
197.086133	4326.468025	6.953805	-0.040035	3.583232
197.295505	4334.515938	6.958810	-0.040080	3.586404
197.481814	4342.513920	6.963814	-0.040120	3.589553
197.520536	4350.567699	6.968819	-0.040133	3.592717
197.781887	4358.615192	6.973824	-0.040188	3.595882
197.981983	4366.573843	6.978829	-0.040231	3.599007
198.259552	4374.620968	6.983834	-0.040288	3.602167
198.696309	4382.576290	6.988838	-0.040375	3.605292
198.807052	4390.629505	6.993843	-0.040401	3.608443
198.952222	4398.719394	6.998848	-0.040434	3.611608
199.068123	4406.713657	7.003853	-0.040461	3.614731
199.628132	4414.754476	7.008858	-0.040571	3.617882
199.789497	4422.775715	7.013862	-0.040607	3.621011
199.779811	4430.782914	7.018867	-0.040611	3.624128
200.162452	4438.832578	7.023872	-0.040688	3.627269
200.301762	4446.837823	7.028877	-0.040720	3.630383
200.639776	4454.898325	7.033882	-0.040788	3.633522
200.861590	4462.954584	7.038886	-0.040835	3.636653
201.081418	4470.911655	7.043891	-0.040882	3.639743
201.320865	4478.959755	7.048896	-0.040932	3.642866
201.447803	4486.936939	7.053901	-0.040962	3.645956
201.866788	4494.969882	7.058906	-0.041045	3.649072
202.082858	4503.020336	7.063910	-0.041091	3.652187
202.381908	4511.045483	7.068915	-0.041153	3.655292
202.842746	4519.059461	7.073920	-0.041244	3.658394
202.918758	4527.110230	7.078925	-0.041264	3.661498
203.198433	4535.079651	7.083930	-0.041322	3.664572
203.467862	4543.132105	7.088934	-0.041378	3.667676
203.715792	4551.174239	7.093939	-0.041430	3.670773
204.045939	4559.214601	7.098944	-0.041497	3.673868
204.061287	4567.232151	7.103949	-0.041505	3.676945
204.368466	4575.217713	7.108954	-0.041568	3.680013
204.506058	4583.249732	7.113958	-0.041600	3.683093
204.581483	4591.273826	7.118963	-0.041619	3.686165
204.964981	4599.310754	7.123968	-0.041697	3.689247
205.279976	4607.331228	7.128973	-0.041761	3.692319
205.409946	4615.377861	7.133978	-0.041791	3.695394
205.625480	4623.364322	7.138982	-0.041837	3.698445
206.071216	4631.351701	7.143987	-0.041925	3.701499
206.058773	4639.367862	7.148992	-0.041929	3.704551
206.100009	4647.406912	7.153997	-0.041942	3.707610
206.619694	4655.456668	7.159002	-0.042045	3.710683
206.847068	4663.555746	7.164006	-0.042093	3.713764
206.918283	4671.585120	7.169011	-0.042112	3.716813
207.153731	4679.555573	7.174016	-0.042161	3.719841
207.306709	4687.525453	7.179021	-0.042195	3.722864
207.638745	4695.542640	7.184026	-0.042263	3.725906
207.672976	4703.576895	7.189030	-0.042275	3.728946
208.017964	4711.568611	7.194035	-0.042345	3.731974
208.216901	4719.633952	7.199040	-0.042388	3.735024
208.209136	4727.660834	7.204045	-0.042392	3.738053
208.471579	4735.688323	7.209050	-0.042447	3.741085
208.760540	4743.676873	7.214054	-0.042506	3.744101
209.167978	4751.692948	7.219059	-0.042588	3.747128
209.311953	4759.735121	7.224064	-0.042620	3.750155
209.569018	4767.764506	7.229069	-0.042674	3.753178
209.847859	4775.837430	7.234074	-0.042731	3.756216
209.869731	4783.832672	7.239078	-0.042741	3.759216
210.057503	4791.846805	7.244083	-0.042782	3.762224
210.540797	4799.822149	7.249088	-0.042878	3.765222
210.462344	4807.872800	7.254093	-0.042869	3.768233
210.550531	4815.940788	7.259098	-0.042891	3.771252
210.960085	4823.958533	7.264102	-0.042973	3.774257
211.006403	4831.997726	7.269107	-0.042987	3.777260
211.256888	4839.991077	7.274112	-0.043039	3.780247
211.464772	4847.985002	7.279117	-0.043084	3.783231
211.788815	4856.017925	7.284122	-0.043150	3.786230
212.046537	4864.039433	7.289126	-0.043204	3.789221
212.210530	4872.103108	7.294131	-0.043240	3.792223
212.415522	4880.167506	7.299136	-0.043284	3.795224
212.510680	4888.092489	7.304141	-0.043307	3.798169
213.044455	4896.121241	7.309146	-0.043412	3.801158
213.314806	4904.082415	7.314150	-0.043468	3.804115
213.156715	4912.176532	7.319155	-0.043445	3.807110
213.560219	4920.179014	7.324160	-0.043525	3.810080
213.763918	4928.208606	7.329165	-0.043569	3.813054
214.256966	4936.218829	7.334170	-0.043667	3.816024
214.226535	4944.239773	7.339174	-0.043667	3.818985
214.229613	4952.267587	7.344179	-0.043673	3.821947
214.639369	4960.257595	7.349184	-0.043755	3.824901
214.677105	4968.293461	7.354189	-0.043768	3.827862
215.006137	4976.345618	7.359194	-0.043835	3.830832
215.184045	4984.363330	7.364198	-0.043874	3.833785
215.410480	4992.401615	7.369203	-0.043921	3.836744
215.697849	5000.380760	7.374208	-0.043981	3.839680
215.590669	5008.405733	7.379213	-0.043966	3.842622
215.845030	5016.414437	7.384218	-0.044019	3.845564
215.969568	5024.448421	7.389222	-0.044048	3.848510
216.381111	5032.489206	7.394227	-0.044131	3.851461
216.621146	5040.519185	7.399232	-0.044181	3.854404
216.616637	5048.581446	7.404237	-0.044186	3.857350
217.096141	5056.569086	7.409242	-0.044281	3.860277
217.305979	5064.588598	7.414246	-0.044326	3.863208
217.279118	5072.584990	7.419251	-0.044326	3.866124
217.591230	5080.650782	7.424256	-0.044390	3.869069
218.068723	5088.689213	7.429261	-0.044485	3.872005
218.632295	5096.931998	7.434266	-0.044596	3.875015
218.773845	5104.843722	7.439270	-0.044628	3.877895
219.002922	5112.725852	7.444275	-0.044676	3.880762
219.325150	5120.738100	7.449280	-0.044742	3.883677
219.371592	5128.749354	7.454285	-0.044756	3.886584
219.398380	5136.777132	7.459290	-0.044767	3.889494
219.771721	5144.759399	7.464294	-0.044842	3.892392
220.072123	5152.824892	7.469299	-0.044904	3.895317
220.112051	5160.848630	7.474304	-0.044917	3.898220
220.151022	5168.861138	7.479309	-0.044930	3.901116
220.555525	5176.854964	7.484314	-0.045011	3.904010
220.723931	5184.915347	7.489318	-0.045048	3.906922
220.830818	5192.880122	7.494323	-0.045073	3.909795
221.159779	5200.937590	7.499328	-0.045140	3.912705
221.166649	5208.974839	7.504333	-0.045147	3.915598
221.390166	5216.970770	7.509338	-0.045195	3.918479
221.871500	5224.974638	7.514342	-0.045290	3.921365
221.845865	5232.957562	7.519347	-0.045291	3.924232
222.031406	5241.040310	7.524352	-0.045331	3.927137
222.214231	5249.008237	7.529357	-0.045371	3.929998
222.542199	5257.079515	7.534362	-0.045438	3.932897
222.410251	5265.099964	7.539366	-0.045419	3.935767
222.654531	5273.069559	7.544371	-0.045470	3.938624
223.037118	5281.142285	7.549376	-0.045547	3.941518
223.292223	5289.103159	7.554381	-0.045600	3.944367
223.371953	5297.177142	7.559386	-0.045621	3.947252
223.678850	5305.168332	7.564390	-0.045684	3.950109
223.893460	5313.246910	7.569395	-0.045729	3.952993
224.000017	5321.305930	7.574400	-0.045755	3.955867
224.187064	5329.242517	7.579405	-0.045795	3.958696
224.652575	5337.261319	7.584410	-0.045888	3.961557
224.895967	5345.222730	7.589414	-0.045939	3.964392
224.900622	5353.256450	7.594419	-0.045945	3.967246
225.008369	5361.282388	7.599424	-0.045971	3.970098
225.133837	5369.305409	7.604429	-0.046000	3.972946
225.283593	5377.379822	7.609434	-0.046034	3.975811
225.677969	5385.385458	7.614438	-0.046113	3.978654
225.755437	5393.394682	7.619443	-0.046133	3.981490
226.214858	5401.424102	7.624448	-0.046224	3.984338
226.160271	5409.452667	7.629453	-0.046220	3.987176
226.543404	5417.459279	7.634458	-0.046297	3.990010
226.527290	5425.543615	7.639462	-0.046300	3.992864
226.741938	5433.543756	7.644467	-0.046345	3.995689
226.915999	5441.590447	7.649472	-0.046384	3.998528
227.048439	5449.537496	7.654477	-0.046414	4.001329
227.283936	5457.569045	7.659482	-0.046463	4.004160
227.349250	5465.592534	7.664486	-0.046481	4.006983
227.797935	5473.590776	7.669491	-0.046571	4.009802
227.861078	5481.703172	7.674496	-0.046588	4.012652
227.947406	5489.710924	7.679501	-0.046610	4.015464
228.251018	5497.705188	7.684506	-0.046672	4.018273
228.407375	5505.705253	7.689510	-0.046707	4.021079
228.533321	5513.718520	7.694515	-0.046736	4.023887
228.905927	5521.753746	7.699520	-0.046811	4.026705
228.998666	5529.763730	7.704525	-0.046834	4.029508
229.311405	5537.829956	7.709530	-0.046898	4.032332
229.705174	5545.881597	7.714534	-0.046977	4.035150
229.940888	5553.843615	7.719539	-0.047027	4.037932
230.269112	5561.827095	7.724544	-0.047093	4.040722
230.309096	5569.834406	7.729549	-0.047107	4.043513
230.490822	5577.846834	7.734554	-0.047146	4.046306
230.639732	5585.856354	7.739558	-0.047180	4.049096
230.811231	5593.893897	7.744563	-0.047217	4.051894
231.297404	5601.922541	7.749568	-0.047313	4.054691
231.492746	5609.921900	7.754573	-0.047356	4.057472
231.522572	5617.964967	7.759578	-0.047367	4.060264
231.404358	5625.960968	7.764582	-0.047351	4.063036
231.745122	5633.969398	7.769587	-0.047420	4.065817
231.916659	5642.003671	7.774592	-0.047457	4.068602
232.044661	5649.991102	7.779597	-0.047487	4.071368
232.421153	5658.046545	7.784602	-0.047563	4.074160
232.596189	5666.083893	7.789606	-0.047601	4.076940
232.722724	5674.026517	7.794611	-0.047630	4.079685
232.791879	5682.127860	7.799616	-0.047649	4.082482
233.068763	5690.063865	7.804621	-0.047706	4.085224
233.328131	5698.146424	7.809626	-0.047760	4.088013
233.573499	5706.157181	7.814630	-0.047811	4.090776
233.744964	5714.174438	7.819635	-0.047849	4.093538
234.219344	5722.233940	7.824640	-0.047943	4.096316
234.241147	5730.181559	7.829645	-0.047953	4.099049
234.446088	5738.260427	7.834650	-0.047997	4.101827
234.637936	5746.225266	7.839654	-0.048038	4.104563
234.725286	5754.270355	7.844659	-0.048060	4.107325
235.123980	5762.299504	7.849664	-0.048140	4.110082
235.291281	5770.338985	7.854669	-0.048177	4.112839
235.557406	5778.384926	7.859674	-0.048232	4.115597
235.421847	5786.381454	7.864678	-0.048213	4.118331
235.629157	5794.374640	7.869683	-0.048257	4.121066
236.057174	5802.401943	7.874688	-0.048342	4.123814
236.001769	5810.409813	7.879693	-0.048338	4.126548
236.312186	5818.435737	7.884698	-0.048401	4.129290
236.640513	5826.472004	7.889702	-0.048468	4.132035
236.928168	5834.451936	7.894707	-0.048527	4.134757
237.218557	5842.511446	7.899712	-0.048587	4.137505
237.246248	5850.490952	7.904717	-0.048598	4.140221
237.597524	5858.557405	7.909722	-0.048669	4.142968
237.498718	5866.539908	7.914726	-0.048657	4.145680
237.797884	5874.576683	7.919731	-0.048718	4.148413
237.920451	5882.627586	7.924736	-0.048747	4.151147
238.121707	5890.666495	7.929741	-0.048790	4.153876
238.338507	5898.695524	7.934746	-0.048836	4.156600
238.598100	5906.653826	7.939750	-0.048890	4.159299
238.670721	5914.670599	7.944755	-0.048909	4.162013
238.957017	5922.664441	7.949760	-0.048968	4.164721
238.997640	5930.706682	7.954765	-0.048981	4.167440
239.164181	5938.701149	7.959770	-0.049018	4.170143
239.527449	5946.762106	7.964774	-0.049091	4.172868
239.591791	5954.778766	7.969779	-0.049109	4.175574
239.951590	5962.790390	7.974784	-0.049182	4.178279
240.197980	5970.778488	7.979789	-0.049233	4.180973
240.165071	5978.811180	7.984794	-0.049233	4.183678
240.493015	5986.807238	7.989798	-0.049300	4.186372
240.653650	5994.827681	7.994803	-0.049335	4.189071
240.963197	6002.885049	7.999808	-0.049399	4.191782
241.180210	6010.965465	8.004813	-0.049445	4.194498
241.322049	6019.004177	8.009818	-0.049477	4.197198
241.359937	6026.914392	8.014822	-0.049490	4.199852
241.631071	6034.928875	8.019827	-0.049546	4.202541
241.814075	6042.920462	8.024832	-0.049586	4.205220
241.898047	6050.927610	8.029837	-0.049607	4.207901
242.139870	6058.978227	8.034842	-0.049658	4.210597
242.473387	6067.013698	8.039846	-0.049726	4.213287
242.699032	6074.993075	8.044851	-0.049773	4.215956
242.860414	6083.016861	8.049856	-0.049809	4.218636
243.005154	6091.012610	8.054861	-0.049842	4.221306
243.496619	6099.018663	8.059866	-0.049939	4.223981
243.701222	6107.044618	8.064870	-0.049983	4.226658
243.819330	6115.081918	8.069875	-0.050010	4.229336
244.281866	6123.104509	8.074880	-0.050102	4.232010
244.391492	6131.140201	8.079885	-0.050128	4.234684
244.672574	6139.156616	8.084890	-0.050186	4.237352
244.670876	6147.164251	8.089894	-0.050192	4.240012
244.767876	6155.162037	8.094899	-0.050216	4.242668
245.143476	6163.172501	8.099904	-0.050291	4.245329
245.505509	6171.196991	8.104909	-0.050364	4.247993
245.499515	6179.242016	8.109914	-0.050369	4.250659
245.498720	6187.306107	8.114918	-0.050375	4.253330
245.930493	6195.270641	8.119923	-0.050461	4.255969
246.422802	6203.327504	8.124928	-0.050558	4.258638
246.573110	6211.349234	8.129933	-0.050592	4.261291
246.592365	6219.343426	8.134938	-0.050601	4.263932
246.745532	6227.401661	8.139942	-0.050635	4.266594
246.910756	6235.375718	8.144947	-0.050672	4.269226
247.144322	6243.480004	8.149952	-0.050721	4.271900
247.171991	6251.458046	8.154957	-0.050732	4.274529
247.325236	6259.493915	8.159962	-0.050766	4.277176
247.367813	6267.449255	8.164966	-0.050780	4.279795
247.686124	6275.510183	8.169971	-0.050845	4.282448
247.724334	6283.470791	8.174976	-0.050857	4.285065
247.817704	6291.510095	8.179981	-0.050881	4.287707
247.891893	6299.512995	8.184986	-0.050900	4.290334
248.335370	6307.569395	8.189990	-0.050988	4.292981
248.620005	6315.573647	8.194995	-0.051047	4.295608
248.801097	6323.602436	8.200000	-0.051086	4.298240
248.834923	6331.580428	8.205005	-0.051098	4.300853
249.201077	6339.610246	8.210010	-0.051172	4.303483
249.295458	6347.622520	8.215014	-0.051196	4.306104
249.361647	6355.643209	8.220019	-0.051214	4.308727
249.638599	6363.687171	8.225024	-0.051271	4.311356
249.575824	6371.727241	8.230029	-0.051265	4.313981
249.728859	6379.733112	8.235034	-0.051299	4.316594
249.941140	6387.698590	8.240038	-0.051344	4.319192
250.103531	6395.740927	8.245043	-0.051380	4.321814
250.270423	6403.732510	8.250048	-0.051417	4.324418
250.322247	6411.763023	8.255053	-0.051432	4.327032
250.746354	6419.777376	8.260058	-0.051517	4.329642
250.924550	6427.802681	8.265062	-0.051556	4.332252
250.967632	6435.801006	8.270067	-0.051570	4.334851
251.409304	6443.908790	8.275072	-0.051658	4.337486
251.438573	6451.856549	8.280077	-0.051669	4.340065
251.500314	6459.860428	8.285082	-0.051686	4.342661
251.899458	6467.880946	8.290086	-0.051766	4.345263
252.251323	6475.876487	8.295091	-0.051837	4.347855
252.320082	6483.941139	8.300096	-0.051856	4.350466
252.222086	6492.029227	8.305101	-0.051843	4.353081
252.543798	6500.039061	8.310106	-0.051909	4.355673
252.785972	6508.011763	8.315110	-0.051960	4.358251
252.718868	6515.963931	8.320115	-0.051953	4.360818
253.114911	6523.987001	8.325120	-0.052032	4.363410
253.366104	6531.935268	8.330125	-0.052085	4.365975
253.370973	6539.982724	8.335130	-0.052091	4.368569
253.422724	6548.064215	8.340134	-0.052107	4.371173
253.645235	6556.063249	8.345139	-0.052154	4.373749
253.769042	6564.111470	8.350144	-0.052183	4.376339
253.728129	6572.050731	8.355149	-0.052181	4.378892
254.034042	6580.121048	8.360154	-0.052243	4.381488
254.287259	6588.104774	8.365158	-0.052296	4.384053
254.422361	6596.114645	8.370163	-0.052327	4.386625
254.721465	6604.139328	8.375168	-0.052389	4.389201
254.904701	6612.206712	8.380173	-0.052428	4.391789
255.203761	6620.244004	8.385178	-0.052490	4.394366
255.411589	6628.246583	8.390182	-0.052534	4.396929
255.599724	6636.186895	8.395187	-0.052575	4.399472
255.750750	6644.273028	8.400192	-0.052609	4.402059
255.868602	6652.256040	8.405197	-0.052636	4.404611
256.090666	6660.293053	8.410202	-0.052683	4.407180
256.321134	6668.264314	8.415206	-0.052732	4.409726
256.478868	6676.312750	8.420211	-0.052767	4.412296
256.569316	6684.370803	8.425216	-0.052790	4.414866
256.612765	6692.398972	8.430221	-0.052804	4.417425
256.889262	6700.385531	8.435226	-0.052861	4.419970
257.024673	6708.449322	8.440230	-0.052892	4.422538
257.169136	6716.374448	8.445235	-0.052924	4.425060
257.450973	6724.482096	8.450240	-0.052982	4.427640
257.323456	6732.464214	8.455245	-0.052964	4.430176
257.855905	6740.549743	8.460250	-0.053069	4.432747
258.076120	6748.538784	8.465254	-0.053116	4.435283
258.231125	6756.543133	8.470259	-0.053151	4.437824
258.585658	6764.502474	8.475264	-0.053222	4.440349
258.692983	6772.521636	8.480269	-0.053248	4.442890
259.133399	6780.502145	8.485274	-0.053336	4.445419
259.085774	6788.607383	8.490278	-0.053333	4.447985
259.271405	6796.536989	8.495283	-0.053373	4.450494
259.650461	6804.660651	8.500288	-0.053449	4.453064
259.525964	6812.625594	8.505293	-0.053432	4.455580
259.730976	6820.661720	8.510298	-0.053475	4.458118
260.156125	6828.625030	8.515302	-0.053560	4.460633
260.193297	6836.642510	8.520307	-0.053573	4.463162
260.349713	6844.678227	8.525312	-0.053608	4.465696
260.388386	6852.700901	8.530317	-0.053621	4.468224
260.878283	6860.720833	8.535322	-0.053718	4.470751
261.047535	6868.779284	8.540326	-0.053755	4.473288
261.332693	6876.739054	8.545331	-0.053814	4.475792
261.429754	6884.771660	8.550336	-0.053837	4.478317
261.486551	6892.743599	8.555341	-0.053854	4.480822
261.855278	6900.779001	8.560346	-0.053928	4.483346
261.957852	6908.808394	8.565351	-0.053953	4.485866
261.946502	6916.819393	8.570355	-0.053956	4.488379
262.142599	6924.865098	8.575360	-0.053999	4.490902
262.376109	6932.850329	8.580365	-0.054048	4.493404
262.629825	6940.908776	8.585370	-0.054101	4.495928
262.638533	6948.914807	8.590375	-0.054108	4.498433
262.633035	6956.900454	8.595379	-0.054113	4.500931
263.019470	6964.936733	8.600384	-0.054191	4.503444
263.084333	6972.901897	8.605389	-0.054208	4.505932
263.348008	6980.959190	8.610394	-0.054263	4.508449
263.683011	6988.996620	8.615399	-0.054331	4.510957
263.695857	6997.055704	8.620403	-0.054339	4.513471
263.801960	7005.079656	8.625408	-0.054365	4.515972
264.175311	7012.999281	8.630413	-0.054440	4.518440
264.475065	7021.018087	8.635418	-0.054501	4.520937
264.489064	7029.031982	8.640423	-0.054510	4.523431
264.530443	7037.030087	8.645427	-0.054523	4.525919
264.890136	7045.042049	8.650432	-0.054596	4.528410
264.916943	7053.064223	8.655437	-0.054607	4.530902
265.086649	7061.105249	8.660442	-0.054644	4.533399
265.256819	7069.170909	8.665447	-0.054681	4.535903
265.161836	7077.131485	8.670451	-0.054669	4.538371
265.484802	7085.187334	8.675456	-0.054735	4.540869
265.564004	7093.142869	8.680461	-0.054756	4.543334
265.708152	7101.157993	8.685466	-0.054788	4.545816
265.826585	7109.184716	8.690471	-0.054816	4.548300
265.943834	7117.175502	8.695475	-0.054843	4.550772
265.976788	7125.305307	8.700480	-0.054855	4.553285
266.115261	7133.302865	8.705485	-0.054887	4.555756
266.371588	7141.303495	8.710490	-0.054940	4.558227
266.445258	7149.304991	8.715495	-0.054960	4.560696
266.679723	7157.287200	8.720499	-0.055009	4.563159
266.958193	7165.278792	8.725504	-0.055067	4.565622
266.985499	7173.338146	8.730509	-0.055077	4.568106
267.176574	7181.336719	8.735514	-0.055119	4.570569
267.345054	7189.376252	8.740519	-0.055156	4.573043
267.513453	7197.393820	8.745523	-0.055193	4.575510
267.691754	7205.449297	8.750528	-0.055232	4.577986
267.747914	7213.393475	8.755533	-0.055248	4.580428
267.926378	7221.454698	8.760538	-0.055287	4.582903
268.220187	7229.442972	8.765543	-0.055347	4.585355
268.594626	7237.478370	8.770547	-0.055423	4.587820
268.678445	7245.514222	8.775552	-0.055444	4.590284
268.728141	7253.523861	8.780557	-0.055459	4.592739
269.107948	7261.582749	8.785562	-0.055535	4.595207
269.499826	7269.620630	8.790567	-0.055614	4.597668
269.592893	7277.521937	8.795571	-0.055637	4.600085
269.711941	7285.605164	8.800576	-0.055665	4.602557
269.863528	7293.545685	8.805581	-0.055699	4.604983
270.142194	7301.593873	8.810586	-0.055756	4.607442
270.197563	7309.614454	8.815591	-0.055772	4.609890
270.235329	7317.627021	8.820595	-0.055785	4.612335
270.366991	7325.661439	8.825600	-0.055815	4.614785
270.601826	7333.702442	8.830605	-0.055865	4.617236
271.061357	7341.618124	8.835610	-0.055956	4.619647
271.040153	7349.712366	8.840615	-0.055958	4.622112
271.104305	7357.708531	8.845619	-0.055976	4.624545
271.219727	7365.734752	8.850624	-0.056003	4.626986
271.383201	7373.715071	8.855629	-0.056039	4.629412
271.545699	7381.764399	8.860634	-0.056075	4.631857
271.726583	7389.778009	8.865639	-0.056114	4.634291
271.984169	7397.815733	8.870643	-0.056168	4.636730
272.361466	7405.805747	8.875648	-0.056244	4.639153
272.294074	7413.825115	8.880653	-0.056237	4.641584
272.613404	7421.759588	8.885658	-0.056302	4.643988
272.948337	7429.839634	8.890663	-0.056370	4.646435
272.917723	7437.837821	8.895667	-0.056370	4.648856
272.961300	7445.918973	8.900672	-0.056384	4.651301
273.125438	7453.896562	8.905677	-0.056420	4.653713
273.524335	7461.935365	8.910682	-0.056500	4.656142
273.625934	7469.913882	8.915687	-0.056525	4.658552
273.782640	7477.904123	8.920691	-0.056560	4.660964
273.954563	7485.992837	8.925696	-0.056598	4.663404
274.113906	7493.948075	8.930701	-0.056633	4.665803
274.193052	7502.016801	8.935706	-0.056653	4.668235
274.456433	7510.038077	8.940711	-0.056708	4.670652
274.728050	7518.079227	8.945715	-0.056764	4.673072
274.786970	7526.185491	8.950720	-0.056781	4.675512
274.786364	7534.068253	8.955725	-0.056787	4.677883
275.203729	7542.032778	8.960730	-0.056870	4.680277
275.500009	7550.093158	8.965735	-0.056931	4.682698
275.545844	7558.001030	8.970739	-0.056945	4.685073
275.740773	7566.096142	8.975744	-0.056987	4.687503
275.852325	7574.067897	8.980749	-0.057014	4.689894
276.043069	7582.130849	8.985754	-0.057055	4.692311
276.072703	7590.198791	8.990759	-0.057066	4.694729
276.220139	7598.172877	8.995763	-0.057099	4.697118
276.448797	7606.129890	9.000768	-0.057148	4.699500
276.614701	7614.179181	9.005773	-0.057184	4.701908
276.656870	7622.183522	9.010778	-0.057198	4.704302
276.734613	7630.234080	9.015783	-0.057218	4.706708
276.884639	7638.209004	9.020787	-0.057252	4.709091
277.429532	7646.272367	9.025792	-0.057359	4.711497
277.310485	7654.304234	9.030797	-0.057342	4.713895
277.474221	7662.336715	9.035802	-0.057379	4.716291
277.506937	7670.317551	9.040807	-0.057390	4.718670
277.694149	7678.282046	9.045811	-0.057431	4.721043
277.997448	7686.328396	9.050816	-0.057493	4.723439
277.880422	7694.336641	9.055821	-0.057477	4.725824
278.228983	7702.392862	9.060826	-0.057548	4.728220
278.380451	7710.397551	9.065831	-0.057581	4.730600
278.330796	7718.416647	9.070835	-0.057578	4.732984
278.807139	7726.446942	9.075840	-0.057672	4.735368
278.648672	7734.446631	9.080845	-0.057649	4.737744
278.861301	7742.469474	9.085850	-0.057694	4.740125
279.204907	7750.504357	9.090855	-0.057764	4.742507
279.417907	7758.451228	9.095859	-0.057809	4.744863
279.606073	7766.525110	9.100864	-0.057850	4.747255
279.675037	7774.508845	9.105869	-0.057868	4.749620
279.961957	7782.556387	9.110874	-0.057927	4.752001
280.159905	7790.604801	9.115879	-0.057970	4.754382
280.450042	7798.601555	9.120883	-0.058030	4.756746
280.589708	7806.520077	9.125888	-0.058061	4.759086
280.776375	7814.588003	9.130893	-0.058102	4.761469
280.904966	7822.556668	9.135898	-0.058131	4.763822
281.154885	7830.622036	9.140903	-0.058184	4.766201
280.953606	7838.607783	9.145907	-0.058152	4.768558
281.332200	7846.631280	9.150912	-0.058228	4.770923
281.375642	7854.668795	9.155917	-0.058242	4.773291
281.559746	7862.675331	9.160922	-0.058282	4.775649
281.744134	7870.735756	9.165927	-0.058322	4.778021
281.854186	7878.664361	9.170931	-0.058348	4.780354
282.127394	7886.730014	9.175936	-0.058405	4.782725
282.175636	7894.668774	9.180941	-0.058419	4.785059
282.243567	7902.767972	9.185946	-0.058438	4.787439
282.532445	7910.802502	9.190951	-0.058497	4.789797
282.661272	7918.778924	9.195955	-0.058527	4.792138
282.879159	7926.834215	9.200960	-0.058573	4.794500
283.145562	7934.815586	9.205965	-0.058629	4.796840
283.265436	7942.812333	9.210970	-0.058657	4.799183
283.319333	7950.879064	9.215975	-0.058672	4.801546
283.431137	7958.816433	9.220979	-0.058699	4.803870
283.733453	7966.881600	9.225984	-0.058761	4.806229
283.966262	7974.917600	9.230989	-0.058810	4.808578
284.081264	7982.854057	9.235994	-0.058837	4.810898
284.407907	7990.406088	9.240999	-0.058903	4.813104
284.700259	7994.962822	9.246003	-0.058961	4.814433

284.714278	7997.589380	9.251008	-0.058966	4.815200
284.844345	7998.878903	9.256013	-0.058991	4.815576
284.963786	7999.364361	9.261018	-0.059014	4.815717
285.043738	8000.413622	9.266023	-0.059031	4.816023
285.032840	8000.428438	9.271027	-0.059029	4.816028
285.415250	8000.422675	9.276032	-0.059101	4.816024
285.416848	8000.400300	9.281037	-0.059101	4.816017
285.338276	8000.438464	9.286042	-0.059087	4.816029
285.579524	8000.449356	9.291047	-0.059133	4.816031
285.650565	8000.421840	9.296051	-0.059146	4.816022
285.513739	8000.449313	9.301056	-0.059121	4.816031
285.459863	8000.467616	9.306061	-0.059112	4.816037
285.707211	8000.464721	9.311066	-0.059158	4.816035
285.840308	8000.454383	9.316071	-0.059184	4.816031
285.765104	8000.428458	9.321075	-0.059170	4.816024
285.877899	8000.507558	9.326080	-0.059192	4.816046
285.871367	8000.487171	9.331085	-0.059191	4.816040
285.797590	8000.502971	9.336090	-0.059178	4.816045
285.897978	8000.481340	9.341095	-0.059197	4.816038
286.003599	8000.446975	9.346099	-0.059217	4.816028
286.129106	8000.501718	9.351104	-0.059241	4.816043
286.186207	8000.482499	9.356109	-0.059252	4.816037
286.141761	8000.478523	9.361114	-0.059244	4.816036
286.390056	8000.497031	9.366119	-0.059291	4.816040
286.263533	8000.477647	9.371123	-0.059268	4.816035
286.401304	8000.516578	9.376128	-0.059294	4.816046
286.260867	8000.490524	9.381133	-0.059268	4.816039
286.375439	8000.465946	9.386138	-0.059290	4.816031
286.301254	8000.523437	9.391143	-0.059277	4.816048
286.477197	8000.494640	9.396147	-0.059310	4.816039
286.686582	8000.529541	9.401152	-0.059350	4.816048
286.526401	8000.493501	9.406157	-0.059320	4.816038
286.598078	8000.538703	9.411162	-0.059334	4.816051
286.624438	8000.529612	9.416167	-0.059339	4.816048
286.684941	8000.519010	9.421171	-0.059351	4.816045
286.504786	8000.538201	9.426176	-0.059318	4.816051
286.650468	8000.479980	9.431181	-0.059346	4.816034
286.492618	8000.503858	9.436186	-0.059317	4.816041
286.617436	8000.515822	9.441191	-0.059340	4.816044
286.549362	8000.466505	9.446195	-0.059328	4.816030
286.599715	8000.526284	9.451200	-0.059338	4.816047
286.474883	8000.495170	9.456205	-0.059315	4.816039
286.540060	8000.496414	9.461210	-0.059328	4.816039
286.555972	8000.478578	9.466215	-0.059331	4.816034
286.499723	8000.471177	9.471219	-0.059321	4.816032
286.777216	8000.500914	9.476224	-0.059374	4.816039
286.733175	8000.501222	9.481229	-0.059366	4.816039
286.769423	8000.496589	9.486234	-0.059373	4.816038
286.603583	8000.490383	9.491239	-0.059343	4.816037
286.618136	8000.463967	9.496243	-0.059346	4.816029
286.825445	8000.515938	9.501248	-0.059385	4.816043
286.688772	8000.522029	9.506253	-0.059360	4.816045
286.807513	8000.436582	9.511258	-0.059383	4.816020
286.871092	8000.520127	9.516263	-0.059395	4.816044
286.722066	8000.515299	9.521267	-0.059368	4.816043
286.802886	8000.530731	9.526272	-0.059383	4.816047
286.886632	8000.503448	9.531277	-0.059399	4.816039
286.788562	8000.543394	9.536282	-0.059382	4.816051
286.921783	8000.527712	9.541287	-0.059407	4.816046
286.665425	8000.499527	9.546291	-0.059360	4.816039
286.804963	8000.542769	9.551296	-0.059386	4.816051
286.765832	8000.480083	9.556301	-0.059379	4.816033
286.657953	8000.463180	9.561306	-0.059360	4.816028
286.935461	8000.503610	9.566311	-0.059412	4.816039
287.092427	8000.462703	9.571315	-0.059441	4.816026
287.026613	8000.531041	9.576320	-0.059430	4.816046
286.984593	8000.522832	9.581325	-0.059422	4.816044
287.122780	8000.547872	9.586330	-0.059449	4.816050
287.222251	8000.526225	9.591335	-0.059468	4.816044
287.169962	8000.502858	9.596339	-0.059458	4.816037
287.254161	8000.518352	9.601344	-0.059475	4.816041
286.950103	8000.480737	9.606349	-0.059418	4.816032
287.222945	8000.522151	9.611354	-0.059470	4.816042
287.416810	8000.530038	9.616359	-0.059506	4.816044
287.286616	8000.511655	9.621363	-0.059482	4.816039
287.107239	8000.547968	9.626368	-0.059450	4.816050
287.346261	8000.491462	9.631373	-0.059495	4.816033
287.282247	8000.532033	9.636378	-0.059483	4.816045
287.043572	8000.534111	9.641383	-0.059439	4.816047
287.057549	8000.537623	9.646387	-0.059442	4.816048
287.194205	8000.558358	9.651392	-0.059468	4.816053
287.098519	8000.508532	9.656397	-0.059451	4.816039
287.078385	8000.505002	9.661402	-0.059448	4.816038
287.372366	8000.531837	9.666407	-0.059503	4.816044
287.263107	8000.482830	9.671411	-0.059483	4.816030
287.309257	8000.493349	9.676416	-0.059492	4.816033
287.387106	8000.534389	9.681421	-0.059507	4.816045
287.410259	8000.558385	9.686426	-0.059512	4.816052
287.450706	8000.536722	9.691431	-0.059520	4.816045
287.404154	8000.543399	9.696435	-0.059512	4.816047
287.823494	8000.503037	9.701440	-0.059590	4.816033
287.611102	8000.555851	9.706445	-0.059551	4.816050
287.552642	8000.536648	9.711450	-0.059541	4.816045
287.590817	8000.550228	9.716455	-0.059548	4.816048
287.406755	8000.547962	9.721459	-0.059515	4.816049
287.566610	8000.557363	9.726464	-0.059545	4.816050
287.601713	8000.513148	9.731469	-0.059552	4.816037
287.544106	8000.519621	9.736474	-0.059542	4.816040
287.540988	8000.557035	9.741479	-0.059541	4.816050
287.601134	8000.550703	9.746483	-0.059553	4.816048
287.824673	8000.531336	9.751488	-0.059595	4.816041
287.533355	8000.529238	9.756493	-0.059541	4.816042
287.593015	8000.557113	9.761498	-0.059553	4.816050
287.728459	8000.550026	9.766503	-0.059579	4.816047
287.680645	8000.550265	9.771507	-0.059570	4.816048
287.554654	8000.558689	9.776512	-0.059547	4.816051
287.804397	8000.537665	9.781517	-0.059594	4.816043
287.712382	8000.539229	9.786522	-0.059578	4.816044
287.730652	8000.521436	9.791527	-0.059582	4.816039
287.708302	8000.537111	9.796531	-0.059578	4.816044
287.724820	8000.570609	9.801536	-0.059582	4.816053
287.547243	8000.526762	9.806541	-0.059549	4.816041
287.379801	8000.536563	9.811546	-0.059518	4.816045
287.589329	8000.553292	9.816551	-0.059558	4.816049
287.722515	8000.524780	9.821555	-0.059583	4.816040
287.745108	8000.574428	9.826560	-0.059588	4.816054
287.530698	8000.559843	9.831565	-0.059548	4.816051
287.627158	8000.560594	9.836570	-0.059567	4.816051
287.867582	8000.537260	9.841575	-0.059612	4.816043
287.795619	8000.543470	9.846579	-0.059599	4.816045
288.019024	8000.570078	9.851584	-0.059641	4.816051
287.847704	8000.557353	9.856589	-0.059610	4.816049
287.753504	8000.562085	9.861594	-0.059593	4.816050
287.954503	8000.567966	9.866599	-0.059631	4.816051
287.795040	8000.543697	9.871603	-0.059601	4.816045
287.816853	8000.583708	9.876608	-0.059606	4.816056
287.851657	8000.557664	9.881613	-0.059613	4.816049
287.974956	8000.562117	9.886618	-0.059636	4.816049
287.891070	8000.554207	9.891623	-0.059621	4.816047
287.675695	8000.463688	9.896627	-0.059581	4.816022
287.959490	8000.571599	9.901632	-0.059635	4.816052
287.884564	8000.533915	9.906637	-0.059621	4.816041
287.710501	8000.556425	9.911642	-0.059589	4.816049
287.814134	8000.535924	9.916647	-0.059609	4.816042
287.846752	8000.535502	9.921651	-0.059616	4.816042
288.098602	8000.533763	9.926656	-0.059663	4.816040
287.859220	8000.505887	9.931661	-0.059619	4.816033
287.742065	8000.542274	9.936666	-0.059598	4.816045
287.940118	8000.521370	9.941671	-0.059635	4.816037
287.979944	8000.512526	9.946675	-0.059643	4.816035
288.108449	8000.564122	9.951680	-0.059667	4.816049
288.006465	8000.539840	9.956685	-0.059649	4.816042
287.950411	8000.529234	9.961690	-0.059639	4.816040
288.222889	8000.577061	9.966695	-0.059690	4.816052
287.991512	8000.545055	9.971699	-0.059648	4.816044
287.790003	8000.572407	9.976704	-0.059611	4.816053
287.770572	8000.532535	9.981709	-0.059607	4.816041
288.036115	8000.570610	9.986714	-0.059657	4.816051
288.127024	8000.547736	9.991719	-0.059675	4.816044
287.837906	8000.545677	9.996723	-0.059621	4.816045
287.986979	8000.574127	10.001728	-0.059650	4.816052
287.999841	8000.536987	10.006733	-0.059652	4.816041
287.868120	8000.535683	10.011738	-0.059628	4.816042
287.910243	8000.558960	10.016743	-0.059637	4.816048
287.921758	8000.525003	10.021747	-0.059639	4.816038
288.226278	8000.527440	10.026752	-0.059697	4.816037
288.092783	8000.508995	10.031757	-0.059672	4.816033
287.960931	8000.485234	10.036762	-0.059648	4.816026
288.190589	8000.551520	10.041767	-0.059691	4.816045
287.975753	8000.569004	10.046771	-0.059652	4.816051
288.181681	8000.558937	10.051776	-0.059691	4.816047
288.162317	8000.499819	10.056781	-0.059688	4.816030
288.176287	8000.535409	10.061786	-0.059691	4.816040
288.012796	8000.553837	10.066791	-0.059661	4.816046
287.977602	8000.519021	10.071795	-0.059655	4.816036
288.169694	8000.494799	10.076800	-0.059691	4.816028
288.073993	8000.516611	10.081805	-0.059674	4.816035
288.227123	8000.546206	10.086810	-0.059703	4.816043
288.341284	8000.571876	10.091815	-0.059724	4.816049
288.186918	8000.528454	10.096819	-0.059696	4.816038
288.144396	8000.528789	10.101824	-0.059689	4.816038
288.216474	8000.519469	10.106829	-0.059702	4.816035
288.449069	8000.539832	10.111834	-0.059746	4.816040
288.236969	8000.561642	10.116839	-0.059707	4.816047
288.180792	8000.541411	10.121843	-0.059697	4.816041
288.207845	8000.551579	10.126848	-0.059703	4.816044
288.157977	8000.540017	10.131853	-0.059694	4.816041
288.308255	8000.531066	10.136858	-0.059722	4.816038
288.302225	8000.547042	10.141863	-0.059722	4.816042
288.146497	8000.555988	10.146867	-0.059693	4.816046
288.292501	8000.577967	10.151872	-0.059721	4.816051
288.235291	8000.553439	10.156877	-0.059711	4.816045
288.228849	8000.529844	10.161882	-0.059710	4.816038
288.440649	8000.563725	10.166887	-0.059750	4.816046
288.335431	8000.542592	10.171891	-0.059731	4.816041
288.436317	8000.535940	10.176896	-0.059750	4.816038
288.187355	8000.513233	10.181901	-0.059704	4.816033
288.121791	8000.487483	10.186906	-0.059693	4.816026
288.371654	8000.559488	10.191911	-0.059740	4.816045
288.312569	8000.554172	10.196915	-0.059729	4.816044
288.291551	8000.555972	10.201920	-0.059726	4.816045
288.361974	8000.562661	10.206925	-0.059739	4.816046
288.400954	8000.526000	10.211930	-0.059747	4.816035
288.211623	8000.562130	10.216935	-0.059712	4.816047
288.200769	8000.519208	10.221939	-0.059711	4.816035
288.351197	8000.482458	10.226944	-0.059739	4.816023
288.190506	8000.516976	10.231949	-0.059710	4.816034
288.245189	8000.552245	10.236954	-0.059720	4.816044
288.433528	8000.552548	10.241959	-0.059756	4.816043
288.342243	8000.555194	10.246963	-0.059739	4.816044
288.324077	8000.543146	10.251968	-0.059737	4.816041
288.241137	8000.534184	10.256973	-0.059722	4.816039
288.409076	8000.509518	10.261978	-0.059753	4.816030
288.586322	8000.557734	10.266983	-0.059787	4.816044
288.338617	8000.535050	10.271987	-0.059741	4.816038
288.519612	8000.552326	10.276992	-0.059775	4.816042
288.522329	8000.532107	10.281997	-0.059776	4.816036
288.304046	8000.553804	10.287002	-0.059736	4.816044
288.231623	8000.564283	10.292007	-0.059723	4.816047
288.304176	8000.568872	10.297011	-0.059737	4.816048
288.286504	8000.580357	10.302016	-0.059734	4.816052
288.343960	8000.556868	10.307021	-0.059746	4.816045
288.456567	8000.562193	10.312026	-0.059767	4.816045
288.354463	8000.549671	10.317031	-0.059748	4.816042
288.374368	8000.498760	10.322035	-0.059753	4.816027
288.464563	8000.530405	10.327040	-0.059770	4.816036
288.402259	8000.531446	10.332045	-0.059759	4.816037
288.282753	8000.543197	10.337050	-0.059737	4.816041
288.229674	8000.580763	10.342055	-0.059728	4.816052
288.446484	8000.567688	10.347059	-0.059769	4.816047
288.560353	8000.549513	10.352064	-0.059790	4.816041
288.531360	8000.531920	10.357069	-0.059785	4.816036
288.537968	8000.514981	10.362074	-0.059787	4.816031
288.614926	8000.548521	10.367079	-0.059802	4.816040
288.487209	8000.510935	10.372083	-0.059778	4.816030
288.664997	8000.561300	10.377088	-0.059812	4.816044
288.510582	8000.531776	10.382093	-0.059784	4.816036
288.477784	8000.553676	10.387098	-0.059778	4.816043
288.650580	8000.563316	10.392103	-0.059811	4.816045
288.624255	8000.546841	10.397107	-0.059806	4.816040
288.512178	8000.554451	10.402112	-0.059786	4.816043
288.362879	8000.530368	10.407117	-0.059759	4.816036
288.611499	8000.530710	10.412122	-0.059806	4.816035
288.905616	8000.548997	10.417127	-0.059861	4.816039
288.693594	8000.518414	10.422131	-0.059822	4.816031
288.787868	8000.559759	10.427136	-0.059840	4.816043
288.778141	8000.561766	10.432141	-0.059838	4.816043
288.663683	8000.545809	10.437146	-0.059818	4.816039
288.707049	8000.468597	10.442151	-0.059826	4.816016
288.698059	8000.499488	10.447155	-0.059825	4.816025
288.738502	8000.538773	10.452160	-0.059833	4.816037
288.669840	8000.522589	10.457165	-0.059821	4.816032
288.543882	8000.566299	10.462170	-0.059798	4.816046
288.577840	8000.527408	10.467175	-0.059805	4.816034
288.596072	8000.520306	10.472179	-0.059808	4.816032
288.545976	8000.529056	10.477184	-0.059800	4.816035
288.658449	8000.527964	10.482189	-0.059821	4.816034
288.541502	8000.526931	10.487194	-0.059800	4.816034
288.568039	8000.549921	10.492199	-0.059805	4.816041
288.583606	8000.458297	10.497203	-0.059808	4.816014
288.519910	8000.505291	10.502208	-0.059797	4.816028
288.527694	8000.481958	10.507213	-0.059799	4.816021
288.739227	8000.494449	10.512218	-0.059839	4.816024
288.678159	8000.531868	10.517223	-0.059828	4.816035
288.483573	8000.534754	10.522227	-0.059792	4.816037
288.748241	8000.576024	10.527232	-0.059842	4.816047
288.474867	8000.506888	10.532237	-0.059792	4.816029
288.472512	8000.520793	10.537242	-0.059792	4.816033
288.625945	8000.561086	10.542247	-0.059821	4.816044
288.529522	8000.557223	10.547251	-0.059803	4.816043
288.824604	8000.561627	10.552256	-0.059859	4.816043
288.532148	8000.562713	10.557261	-0.059805	4.816045
288.757169	8000.539097	10.562266	-0.059847	4.816036
288.866240	8000.551843	10.567271	-0.059868	4.816040
288.612817	8000.523706	10.572275	-0.059821	4.816033
288.496480	8000.535516	10.577280	-0.059800	4.816037
288.631108	8000.529485	10.582285	-0.059826	4.816034
288.597463	8000.546022	10.587290	-0.059820	4.816039
288.752229	8000.542500	10.592295	-0.059849	4.816037
288.759716	8000.521300	10.597299	-0.059851	4.816031
288.661141	8000.585830	10.602304	-0.059833	4.816050
288.521576	8000.572619	10.607309	-0.059808	4.816047
288.709754	8000.596443	10.612314	-0.059843	4.816053
288.826668	8000.591156	10.617319	-0.059865	4.816051
288.695673	8000.517153	10.622323	-0.059841	4.816030
288.483139	8000.535747	10.627328	-0.059802	4.816037
288.700219	8000.498085	10.632333	-0.059843	4.816025
288.674894	8000.480558	10.637338	-0.059839	4.816020
288.757117	8000.529166	10.642343	-0.059855	4.816033
288.629407	8000.541835	10.647347	-0.059832	4.816038
288.814441	8000.550632	10.652352	-0.059866	4.816039
288.681919	8000.553589	10.657357	-0.059842	4.816041
288.779643	8000.559711	10.662362	-0.059861	4.816042
288.957282	8000.555541	10.667367	-0.059895	4.816040
288.741683	8000.499229	10.672371	-0.059855	4.816025
288.728108	8000.552491	10.677376	-0.059853	4.816040
288.768769	8000.559702	10.682381	-0.059861	4.816042
288.739315	8000.546377	10.687386	-0.059856	4.816038
288.755616	8000.582011	10.692391	-0.059859	4.816049
288.675810	8000.568829	10.697395	-0.059845	4.816045
288.807324	8000.554186	10.702400	-0.059870	4.816040
288.714852	8000.558949	10.707405	-0.059853	4.816042
288.699867	8000.551236	10.712410	-0.059851	4.816040
288.842492	8000.550699	10.717415	-0.059878	4.816039
288.830325	8000.531276	10.722419	-0.059876	4.816033
288.671438	8000.559411	10.727424	-0.059847	4.816042
288.726338	8000.525182	10.732429	-0.059858	4.816032
288.735005	8000.496518	10.737434	-0.059860	4.816024
288.841856	8000.544510	10.742439	-0.059880	4.816037
288.705899	8000.488594	10.747443	-0.059855	4.816021
288.807646	8000.550392	10.752448	-0.059875	4.816039
288.765210	8000.518650	10.757453	-0.059867	4.816030
288.766538	8000.483436	10.762458	-0.059868	4.816020
288.966777	8000.549185	10.767463	-0.059906	4.816038
288.866473	8000.516378	10.772467	-0.059888	4.816029
288.966155	8000.577070	10.777472	-0.059907	4.816046
288.583645	8000.543351	10.782477	-0.059836	4.816038
288.583154	8000.526281	10.787482	-0.059836	4.816033
288.623721	8000.522798	10.792487	-0.059844	4.816032
288.716389	8000.513857	10.797491	-0.059862	4.816029
288.750583	8000.587245	10.802496	-0.059869	4.816050
288.741473	8000.540076	10.807501	-0.059868	4.816036
288.783110	8000.507742	10.812506	-0.059876	4.816026
288.896908	8000.554792	10.817511	-0.059898	4.816040
288.787779	8000.490815	10.822515	-0.059878	4.816021
288.733454	8000.547605	10.827520	-0.059868	4.816038
288.690955	8000.511585	10.832525	-0.059861	4.816028
288.883601	8000.433909	10.837530	-0.059897	4.816004
289.101773	8000.525651	10.842535	-0.059938	4.816030
288.808969	8000.536353	10.847539	-0.059884	4.816035
288.854767	8000.452769	10.852544	-0.059893	4.816010
288.842675	8000.539207	10.857549	-0.059892	4.816035
288.725557	8000.564902	10.862554	-0.059870	4.816043
288.830271	8000.549767	10.867559	-0.059890	4.816038
288.673633	8000.541588	10.872563	-0.059862	4.816037
288.724559	8000.572512	10.877568	-0.059872	4.816045
288.678059	8000.511824	10.882573	-0.059863	4.816028
288.790371	8000.541739	10.887578	-0.059885	4.816036
288.853733	8000.575031	10.892583	-0.059897	4.816045
288.793435	8000.526921	10.897587	-0.059886	4.816032
288.974490	8000.564515	10.902592	-0.059920	4.816042
289.021303	8000.542969	10.907597	-0.059930	4.816035
288.964740	8000.505620	10.912602	-0.059920	4.816025
288.946274	8000.549170	10.917607	-0.059917	4.816037
288.866969	8000.519957	10.922611	-0.059902	4.816029
288.897203	8000.579372	10.927616	-0.059908	4.816046
288.877641	8000.539496	10.932621	-0.059905	4.816035
288.983272	8000.546833	10.937626	-0.059925	4.816036
288.875136	8000.528853	10.942631	-0.059906	4.816032
288.849286	8000.503831	10.947635	-0.059901	4.816025
288.967792	8000.553107	10.952640	-0.059924	4.816038
288.972353	8000.552169	10.957645	-0.059925	4.816038
288.821441	8000.509878	10.962650	-0.059898	4.816026
288.844419	8000.539219	10.967655	-0.059903	4.816035
288.795486	8000.507358	10.972659	-0.059894	4.816026
288.973829	8000.504269	10.977664	-0.059928	4.816024
288.806720	8000.531184	10.982669	-0.059897	4.816033
288.837541	8000.475126	10.987674	-0.059903	4.816016
288.941055	8000.548720	10.992679	-0.059923	4.816037
288.679297	8000.514014	10.997683	-0.059875	4.816028
289.010882	8000.538337	11.002688	-0.059937	4.816034
289.027161	8000.527992	11.007693	-0.059940	4.816030
288.933058	8000.512408	11.012698	-0.059923	4.816026
289.186820	8000.555617	11.017703	-0.059971	4.816038
289.065178	8000.489270	11.022707	-0.059949	4.816019
288.974903	8000.547538	11.027712	-0.059933	4.816036
288.853938	8000.542153	11.032717	-0.059911	4.816035
289.025409	8000.518622	11.037722	-0.059943	4.816028
289.045112	8000.555388	11.042727	-0.059947	4.816038
289.026527	8000.580757	11.047731	-0.059944	4.816046
289.011777	8000.602989	11.052736	-0.059942	4.816052
289.016705	8000.482297	11.057741	-0.059943	4.816017
288.978768	8000.580022	11.062746	-0.059937	4.816046
288.901087	8000.558324	11.067751	-0.059923	4.816040
288.908399	8000.505042	11.072755	-0.059925	4.816024
289.099963	8000.541761	11.077760	-0.059961	4.816034
289.026106	8000.542589	11.082765	-0.059947	4.816035
288.915084	8000.525624	11.087770	-0.059927	4.816030
288.959120	8000.563907	11.092775	-0.059936	4.816041
288.843203	8000.515843	11.097779	-0.059915	4.816028
288.971835	8000.508633	11.102784	-0.059939	4.816025
289.142371	8000.520372	11.107789	-0.059971	4.816027
288.901627	8000.499952	11.112794	-0.059927	4.816023
289.117026	8000.560634	11.117799	-0.059968	4.816039
289.255127	8000.505480	11.122803	-0.059994	4.816022
289.133884	8000.556763	11.127808	-0.059972	4.816038
288.980173	8000.535805	11.132813	-0.059944	4.816033
288.925915	8000.543409	11.137818	-0.059934	4.816035
289.092012	8000.573244	11.142823	-0.059966	4.816043
289.135524	8000.544152	11.147827	-0.059974	4.816034
289.270493	8000.583039	11.152832	-0.060000	4.816045
289.172228	8000.536368	11.157837	-0.059982	4.816032
289.126327	8000.521671	11.162842	-0.059974	4.816028
289.018243	8000.578542	11.167847	-0.059954	4.816045
289.091458	8000.528610	11.172851	-0.059968	4.816030
289.126089	8000.604146	11.177856	-0.059975	4.816052
288.823214	8000.572959	11.182861	-0.059919	4.816044
288.947360	8000.492955	11.187866	-0.059943	4.816020
288.956558	8000.514558	11.192871	-0.059945	4.816026
288.796181	8000.526626	11.197875	-0.059916	4.816031
289.118141	8000.583921	11.202880	-0.059976	4.816046
289.162689	8000.535601	11.207885	-0.059985	4.816031
289.055529	8000.537955	11.212890	-0.059965	4.816033
288.868777	8000.548468	11.217895	-0.059931	4.816037
288.981167	8000.548445	11.222899	-0.059953	4.816036
289.117288	8000.564897	11.227904	-0.059978	4.816040
289.193029	8000.459408	11.232909	-0.059993	4.816009
289.019573	8000.540740	11.237914	-0.059961	4.816034
289.193578	8000.556820	11.242919	-0.059994	4.816037
289.050794	8000.542479	11.247923	-0.059968	4.816034
289.238474	8000.551325	11.252928	-0.060003	4.816035
289.176600	8000.564136	11.257933	-0.059992	4.816040
289.229895	8000.561956	11.262938	-0.060003	4.816039
289.129632	8000.577268	11.267943	-0.059985	4.816044
289.000003	8000.569585	11.272947	-0.059961	4.816042
289.032628	8000.596965	11.277952	-0.059968	4.816050
288.845965	8000.521937	11.282957	-0.059933	4.816029
288.809645	8000.539494	11.287962	-0.059927	4.816034
289.042416	8000.599427	11.292967	-0.059971	4.816050
289.011882	8000.580735	11.297971	-0.059966	4.816045
289.031083	8000.558680	11.302976	-0.059970	4.816039
289.024814	8000.545781	11.307981	-0.059969	4.816035
289.123530	8000.552991	11.312986	-0.059988	4.816036
289.049370	8000.573061	11.317991	-0.059974	4.816043
289.120074	8000.514528	11.322995	-0.059988	4.816025
289.233696	8000.574408	11.328000	-0.060010	4.816042
289.075460	8000.558714	11.333005	-0.059981	4.816038
288.883527	8000.559508	11.338010	-0.059946	4.816040
289.300544	8000.591821	11.343015	-0.060024	4.816047
289.079765	8000.533273	11.348019	-0.059983	4.816031
288.986879	8000.544444	11.353024	-0.059966	4.816035
288.836906	8000.555634	11.358029	-0.059939	4.816039
289.040958	8000.512386	11.363034	-0.059977	4.816025
288.993048	8000.517968	11.368039	-0.059969	4.816027
289.046035	8000.453763	11.373043	-0.059979	4.816008
289.174582	8000.456175	11.378048	-0.060004	4.816008
289.071033	8000.534516	11.383053	-0.059985	4.816031
289.205264	8000.559488	11.388058	-0.060010	4.816038
289.345647	8000.585643	11.393063	-0.060037	4.816045
289.349120	8000.544051	11.398067	-0.060038	4.816032
289.247001	8000.580716	11.403072	-0.060020	4.816044
289.018243	8000.563724	11.408077	-0.059977	4.816040
289.166123	8000.559006	11.413082	-0.060005	4.816038
289.131756	8000.564838	11.418087	-0.059999	4.816040
289.078239	8000.547861	11.423091	-0.059990	4.816035
289.327585	8000.542872	11.428096	-0.060037	4.816032
289.256854	8000.549104	11.433101	-0.060024	4.816034
289.046030	8000.543135	11.438106	-0.059985	4.816034
289.147466	8000.566435	11.443111	-0.060005	4.816040
289.043480	8000.530352	11.448115	-0.059986	4.816030
289.010322	8000.512681	11.453120	-0.059980	4.816025
289.230957	8000.522134	11.458125	-0.060022	4.816026
289.124762	8000.488149	11.463130	-0.060002	4.816017
289.205837	8000.550638	11.468135	-0.060018	4.816035
289.075594	8000.508726	11.473139	-0.059994	4.816023
289.232249	8000.549081	11.478144	-0.060024	4.816034
289.362000	8000.521575	11.483149	-0.060049	4.816025
289.354118	8000.520408	11.488154	-0.060048	4.816025
289.175104	8000.550311	11.493159	-0.060015	4.816035
289.145071	8000.538044	11.498163	-0.060010	4.816031
289.143536	8000.564796	11.503168	-0.060010	4.816039
289.236328	8000.528056	11.508173	-0.060028	4.816028
289.148127	8000.495472	11.513178	-0.060012	4.816019
289.184094	8000.548577	11.518183	-0.060019	4.816034
289.052526	8000.518402	11.523187	-0.059995	4.816026
289.234035	8000.561353	11.528192	-0.060029	4.816038
289.180776	8000.545451	11.533197	-0.060020	4.816033
289.058620	8000.475886	11.538202	-0.059997	4.816014
289.251004	8000.577848	11.543207	-0.060034	4.816042
289.252519	8000.549052	11.548211	-0.060035	4.816034
289.261133	8000.535358	11.553216	-0.060037	4.816030
289.040707	8000.526004	11.558221	-0.059996	4.816028
289.211306	8000.497111	11.563226	-0.060028	4.816019
289.429074	8000.562115	11.568231	-0.060069	4.816037
289.074581	8000.533186	11.573235	-0.060004	4.816030
289.272855	8000.546505	11.578240	-0.060041	4.816033
289.590129	8000.550251	11.583245	-0.060101	4.816032
289.486959	8000.430777	11.588250	-0.060082	4.815998
289.269133	8000.569035	11.593255	-0.060042	4.816040
289.201552	8000.543246	11.598259	-0.060030	4.816032
289.182522	8000.598547	11.603264	-0.060027	4.816049
289.286087	8000.582322	11.608269	-0.060047	4.816043
289.196835	8000.588213	11.613274	-0.060030	4.816045
289.295760	8000.610397	11.618279	-0.060049	4.816051
289.157359	8000.541602	11.623283	-0.060024	4.816032
289.287192	8000.610335	11.628288	-0.060049	4.816051
289.445603	8000.493534	11.633293	-0.060079	4.816016
289.356848	8000.581771	11.638298	-0.060063	4.816043
289.621572	8000.599522	11.643303	-0.060112	4.816046
289.522937	8000.538942	11.648307	-0.060095	4.816029
289.676935	8000.552516	11.653312	-0.060124	4.816032
289.520260	8000.555028	11.658317	-0.060095	4.816034
289.310009	8000.527683	11.663322	-0.060056	4.816027
289.458794	8000.563616	11.668327	-0.060085	4.816037
289.396348	8000.560377	11.673331	-0.060073	4.816036
289.546573	8000.499029	11.678336	-0.060102	4.816017
289.431947	8000.553642	11.683341	-0.060081	4.816034
289.417890	8000.580164	11.688346	-0.060079	4.816042
289.520109	8000.612033	11.693351	-0.060098	4.816050
289.177232	8000.557654	11.698355	-0.060035	4.816036
289.374656	8000.566680	11.703360	-0.060072	4.816038
289.267975	8000.551933	11.708365	-0.060053	4.816034
289.392341	8000.543576	11.713370	-0.060076	4.816031
289.416778	8000.567598	11.718375	-0.060082	4.816038
289.307044	8000.549587	11.723379	-0.060062	4.816033
289.529123	8000.580454	11.728384	-0.060103	4.816041
289.458384	8000.558883	11.733389	-0.060091	4.816035
289.568638	8000.525672	11.738394	-0.060112	4.816025
289.531651	8000.479058	11.743399	-0.060105	4.816011
289.446986	8000.513905	11.748403	-0.060090	4.816022
289.516744	8000.553732	11.753408	-0.060104	4.816033
289.467879	8000.555019	11.758413	-0.060095	4.816034
289.269547	8000.505438	11.763418	-0.060058	4.816020
289.433096	8000.559821	11.768423	-0.060089	4.816035
289.429076	8000.518092	11.773427	-0.060089	4.816023
289.548341	8000.537442	11.778432	-0.060112	4.816028
289.546978	8000.552436	11.783437	-0.060112	4.816033
289.530208	8000.523303	11.788442	-0.060109	4.816024
289.523370	8000.590592	11.793447	-0.060109	4.816044
289.491667	8000.546215	11.798451	-0.060103	4.816031
289.442780	8000.553917	11.803456	-0.060095	4.816034
289.312979	8000.528052	11.808461	-0.060071	4.816027
289.322955	8000.469471	11.813466	-0.060073	4.816010
289.426001	8000.549475	11.818471	-0.060093	4.816032
289.530779	8000.538618	11.823475	-0.060113	4.816029
289.541377	8000.557039	11.828480	-0.060115	4.816034
289.687007	8000.551212	11.833485	-0.060143	4.816031
289.522824	8000.497981	11.838490	-0.060113	4.816017
289.342890	8000.566363	11.843495	-0.060080	4.816038
289.478423	8000.548587	11.848499	-0.060106	4.816032
289.609125	8000.548901	11.853504	-0.060130	4.816031
289.705293	8000.550718	11.858509	-0.060149	4.816031
289.396849	8000.478793	11.863514	-0.060092	4.816012
289.587481	8000.519774	11.868519	-0.060128	4.816023
289.492963	8000.488142	11.873523	-0.060111	4.816014
289.701465	8000.543353	11.878528	-0.060150	4.816029
289.500218	8000.525797	11.883533	-0.060113	4.816025
289.474054	8000.530710	11.888538	-0.060109	4.816026
289.553983	8000.568585	11.893543	-0.060124	4.816037
289.589487	8000.514751	11.898547	-0.060131	4.816021
289.814047	8000.532831	11.903552	-0.060173	4.816025
289.517568	8000.553088	11.908557	-0.060119	4.816033
289.554299	8000.432979	11.913562	-0.060126	4.815997
289.508473	8000.576541	11.918567	-0.060118	4.816040
289.483372	8000.539770	11.923571	-0.060114	4.816029
289.529776	8000.559919	11.928576	-0.060123	4.816035
289.597187	8000.529128	11.933581	-0.060136	4.816025
289.665227	8000.543259	11.938586	-0.060149	4.816029
289.626137	8000.603539	11.943591	-0.060142	4.816047
289.552217	8000.502780	11.948595	-0.060129	4.816018
289.588985	8000.559109	11.953600	-0.060136	4.816034
289.653522	8000.563552	11.958605	-0.060149	4.816035
289.546092	8000.553068	11.963610	-0.060129	4.816032
289.489892	8000.554221	11.968615	-0.060119	4.816033
289.655170	8000.511329	11.973619	-0.060151	4.816020
289.586410	8000.530428	11.978624	-0.060138	4.816025
289.683345	8000.530121	11.983629	-0.060157	4.816025
289.630981	8000.490710	11.988634	-0.060147	4.816014
289.617227	8000.557872	11.993639	-0.060145	4.816033
289.646447	8000.540278	11.998643	-0.060151	4.816028
289.630103	8000.486559	12.003648	-0.060149	4.816012
289.721869	8000.548178	12.008653	-0.060166	4.816030
289.524357	8000.526413	12.013658	-0.060130	4.816025
289.672902	8000.578382	12.018663	-0.060158	4.816039
289.532806	8000.522386	12.023667	-0.060133	4.816023
289.685850	8000.539151	12.028672	-0.060162	4.816027
289.635858	8000.570359	12.033677	-0.060153	4.816037
289.737358	8000.515600	12.038682	-0.060172	4.816020
289.627556	8000.546776	12.043687	-0.060152	4.816030
289.579324	8000.524550	12.048691	-0.060144	4.816024
289.800288	8000.582130	12.053696	-0.060185	4.816039
289.701773	8000.547216	12.058701	-0.060167	4.816030
289.451516	8000.527688	12.063706	-0.060121	4.816025
289.605911	8000.562657	12.068711	-0.060151	4.816035
289.469759	8000.509941	12.073715	-0.060126	4.816020
289.500992	8000.515910	12.078720	-0.060132	4.816021
289.563223	8000.572708	12.083725	-0.060144	4.816038
289.502117	8000.560938	12.088730	-0.060133	4.816035
289.506371	8000.497974	12.093735	-0.060134	4.816016
289.358502	8000.522034	12.098739	-0.060107	4.816024
289.393399	8000.589021	12.103744	-0.060114	4.816043
289.240739	8000.567013	12.108749	-0.060086	4.816038
289.417603	8000.537166	12.113754	-0.060120	4.816028
289.510645	8000.556034	12.118759	-0.060138	4.816033
289.609877	8000.535452	12.123763	-0.060157	4.816026
289.552936	8000.583641	12.128768	-0.060147	4.816041
289.541933	8000.553545	12.133773	-0.060145	4.816032
289.513483	8000.560555	12.138778	-0.060140	4.816034
289.636427	8000.471972	12.143783	-0.060163	4.816008
289.414907	8000.527826	12.148787	-0.060123	4.816025
289.730393	8000.578591	12.153792	-0.060182	4.816038
289.740089	8000.562777	12.158797	-0.060184	4.816034
289.539276	8000.525980	12.163802	-0.060147	4.816024
289.505856	8000.538245	12.168807	-0.060142	4.816028
289.424417	8000.519685	12.173811	-0.060127	4.816023
289.524611	8000.523715	12.178816	-0.060146	4.816023
289.594690	8000.538954	12.183821	-0.060160	4.816027
289.543684	8000.485666	12.188826	-0.060151	4.816012
289.651640	8000.517641	12.193831	-0.060171	4.816021
289.466815	8000.486486	12.198835	-0.060137	4.816013
289.615641	8000.540599	12.203840	-0.060165	4.816028
289.777049	8000.532924	12.208845	-0.060196	4.816025
289.686135	8000.452169	12.213850	-0.060179	4.816001
289.607057	8000.529891	12.218855	-0.060165	4.816025
289.521746	8000.525161	12.223859	-0.060150	4.816024
289.759693	8000.588401	12.228864	-0.060195	4.816041
289.589429	8000.536126	12.233869	-0.060163	4.816026
289.602216	8000.490428	12.238874	-0.060166	4.816013
289.575592	8000.544522	12.243879	-0.060162	4.816029
289.558728	8000.534635	12.248883	-0.060159	4.816026
289.393569	8000.543406	12.253888	-0.060129	4.816030
289.471787	8000.545963	12.258893	-0.060144	4.816030
289.348569	8000.503109	12.263898	-0.060121	4.816018
289.433505	8000.457670	12.268903	-0.060138	4.816004
289.608236	8000.483388	12.273907	-0.060171	4.816011
289.572316	8000.498815	12.278912	-0.060165	4.816015
289.496106	8000.535956	12.283917	-0.060151	4.816027
289.625894	8000.550154	12.288922	-0.060176	4.816030
289.657955	8000.604258	12.293927	-0.060182	4.816046
289.468769	8000.538804	12.298931	-0.060147	4.816028
289.662002	8000.540268	12.303936	-0.060184	4.816027
289.742294	8000.564250	12.308941	-0.060199	4.816034
289.667660	8000.570409	12.313946	-0.060186	4.816036
289.645949	8000.493066	12.318951	-0.060182	4.816013
289.562022	8000.564283	12.323955	-0.060167	4.816035
289.589389	8000.559488	12.328960	-0.060173	4.816033
289.490257	8000.558781	12.333965	-0.060155	4.816033
289.658828	8000.540544	12.338970	-0.060186	4.816027
289.827470	8000.576845	12.343975	-0.060218	4.816037
289.465042	8000.531727	12.348979	-0.060151	4.816025
289.469308	8000.577834	12.353984	-0.060153	4.816039
289.707914	8000.475340	12.358989	-0.060198	4.816008
289.557245	8000.535706	12.363994	-0.060170	4.816026
289.674411	8000.578544	12.368999	-0.060192	4.816038
289.722844	8000.550611	12.374003	-0.060202	4.816030
289.757363	8000.516006	12.379008	-0.060209	4.816019
289.829725	8000.522732	12.384013	-0.060223	4.816021
289.592210	8000.477775	12.389018	-0.060179	4.816009
289.731329	8000.543473	12.394023	-0.060205	4.816027
289.564684	8000.557563	12.399027	-0.060175	4.816032
289.565128	8000.520193	12.404032	-0.060175	4.816021
289.595044	8000.505820	12.409037	-0.060181	4.816017
289.592948	8000.513315	12.414042	-0.060181	4.816019
289.610244	8000.496572	12.419047	-0.060185	4.816014
289.740288	8000.565311	12.424051	-0.060210	4.816034
289.532839	8000.560472	12.429056	-0.060172	4.816033
289.558414	8000.543881	12.434061	-0.060177	4.816028
289.552201	8000.567339	12.439066	-0.060176	4.816035
289.662234	8000.559788	12.444071	-0.060197	4.816032
289.617388	8000.520515	12.449075	-0.060189	4.816021
289.529894	8000.480457	12.454080	-0.060174	4.816010
289.609692	8000.555756	12.459085	-0.060189	4.816031
289.635222	8000.499599	12.464090	-0.060194	4.816015
289.518209	8000.540267	12.469095	-0.060173	4.816027
289.521048	8000.507218	12.474099	-0.060174	4.816018
289.621673	8000.545474	12.479104	-0.060193	4.816028
289.542783	8000.547278	12.484109	-0.060179	4.816029
289.609288	8000.543203	12.489114	-0.060192	4.816028
289.508273	8000.601275	12.494119	-0.060173	4.816045
289.556425	8000.571198	12.499123	-0.060183	4.816036
289.425385	8000.495051	12.504128	-0.060159	4.816015
289.372505	8000.573256	12.509133	-0.060150	4.816038
289.422218	8000.538930	12.514138	-0.060159	4.816027
289.618048	8000.591771	12.519143	-0.060196	4.816042
289.404201	8000.536556	12.524147	-0.060157	4.816027
289.665665	8000.572425	12.529152	-0.060206	4.816036
289.673950	8000.563001	12.534157	-0.060208	4.816033
289.579660	8000.540997	12.539162	-0.060191	4.816027
289.684292	8000.549386	12.544167	-0.060211	4.816029
289.646030	8000.463183	12.549171	-0.060204	4.816004
289.643817	8000.518795	12.554176	-0.060204	4.816020
289.779279	8000.558763	12.559181	-0.060230	4.816031
289.634696	8000.512307	12.564186	-0.060204	4.816018
289.715949	8000.471077	12.569191	-0.060219	4.816006
289.587297	8000.476243	12.574195	-0.060196	4.816008
289.698909	8000.548920	12.579200	-0.060217	4.816029
289.788411	8000.576279	12.584205	-0.060234	4.816036
289.753501	8000.579961	12.589210	-0.060228	4.816037
289.893136	8000.572955	12.594215	-0.060255	4.816035
289.919048	8000.512527	12.599219	-0.060260	4.816017
289.653013	8000.539759	12.604224	-0.060211	4.816026
289.626033	8000.553212	12.609229	-0.060206	4.816030
289.717055	8000.445863	12.614234	-0.060224	4.815998
289.978848	8000.477461	12.619239	-0.060273	4.816006
289.887331	8000.553886	12.624243	-0.060257	4.816029
289.886066	8000.503652	12.629248	-0.060257	4.816014
289.943746	8000.558228	12.634253	-0.060268	4.816030
289.827451	8000.550789	12.639258	-0.060247	4.816028
289.893272	8000.502859	12.644263	-0.060260	4.816014
289.723838	8000.527591	12.649267	-0.060229	4.816022
289.767189	8000.604359	12.654272	-0.060237	4.816044
289.802734	8000.583674	12.659277	-0.060244	4.816038
289.817523	8000.579717	12.664282	-0.060247	4.816037
289.922058	8000.503627	12.669287	-0.060267	4.816014
289.642199	8000.550922	12.674291	-0.060216	4.816029
289.804748	8000.538990	12.679296	-0.060247	4.816025
289.763593	8000.598164	12.684301	-0.060239	4.816042
289.836142	8000.461602	12.689306	-0.060253	4.816002
289.993867	8000.592873	12.694311	-0.060283	4.816040
289.852057	8000.510111	12.699315	-0.060257	4.816016
289.895408	8000.556938	12.704320	-0.060266	4.816030
289.822562	8000.531050	12.709325	-0.060253	4.816022
289.963345	8000.517649	12.714330	-0.060279	4.816018
290.093306	8000.587457	12.719335	-0.060304	4.816037
289.827911	8000.551609	12.724339	-0.060255	4.816028
289.781292	8000.525135	12.729344	-0.060247	4.816021
289.920691	8000.473212	12.734349	-0.060273	4.816005
289.866972	8000.513975	12.739354	-0.060264	4.816017
289.912924	8000.581168	12.744359	-0.060273	4.816036
289.776180	8000.525232	12.749363	-0.060248	4.816021
289.784525	8000.528641	12.754368	-0.060250	4.816022
289.812712	8000.529207	12.759373	-0.060256	4.816022
289.739496	8000.564265	12.764378	-0.060243	4.816032
289.933818	8000.576444	12.769383	-0.060279	4.816035
289.702516	8000.515560	12.774387	-0.060237	4.816018
289.785633	8000.540663	12.779392	-0.060253	4.816025
289.938209	8000.533895	12.784397	-0.060282	4.816022
289.719014	8000.479650	12.789402	-0.060241	4.816008
289.840319	8000.522564	12.794407	-0.060264	4.816020
289.998942	8000.494521	12.799411	-0.060294	4.816010
289.906733	8000.536714	12.804416	-0.060278	4.816023
289.886220	8000.521414	12.809421	-0.060274	4.816019
289.778948	8000.473506	12.814426	-0.060255	4.816005
290.004650	8000.494817	12.819431	-0.060297	4.816010
289.890859	8000.528058	12.824435	-0.060277	4.816021
289.737409	8000.552015	12.829440	-0.060248	4.816029
289.821436	8000.556818	12.834445	-0.060265	4.816030
289.768784	8000.494944	12.839450	-0.060255	4.816012
289.914856	8000.520136	12.844455	-0.060283	4.816018
290.011338	8000.521960	12.849459	-0.060301	4.816018
290.032425	8000.507425	12.854464	-0.060306	4.816014
289.977617	8000.559931	12.859469	-0.060296	4.816030
290.147554	8000.548136	12.864474	-0.060328	4.816025
290.124261	8000.586251	12.869479	-0.060324	4.816036
290.014968	8000.516919	12.874483	-0.060304	4.816017
289.994395	8000.541183	12.879488	-0.060301	4.816024
290.157566	8000.561343	12.884493	-0.060332	4.816029
290.011493	8000.408995	12.889498	-0.060305	4.815985
289.941106	8000.526444	12.894503	-0.060293	4.816020
289.888614	8000.523387	12.899507	-0.060283	4.816019
289.954521	8000.518231	12.904512	-0.060296	4.816017
289.739419	8000.551747	12.909517	-0.060257	4.816028
289.734868	8000.579514	12.914522	-0.060256	4.816036
289.782945	8000.615735	12.919527	-0.060266	4.816047
289.653893	8000.548177	12.924531	-0.060242	4.816028
289.671515	8000.565659	12.929536	-0.060246	4.816033
289.823866	8000.563164	12.934541	-0.060275	4.816031
289.785506	8000.534703	12.939546	-0.060268	4.816023
289.723172	8000.559268	12.944551	-0.060257	4.816030
289.846805	8000.528441	12.949555	-0.060280	4.816021
290.060887	8000.441535	12.954560	-0.060321	4.815994
289.932616	8000.539740	12.959565	-0.060297	4.816024
289.876267	8000.501324	12.964570	-0.060287	4.816013
289.931447	8000.514150	12.969575	-0.060298	4.816016
289.945200	8000.514451	12.974579	-0.060301	4.816016
289.837860	8000.560643	12.979584	-0.060282	4.816030
289.828926	8000.590468	12.984589	-0.060281	4.816039
290.019675	8000.538421	12.989594	-0.060316	4.816023
289.860979	8000.579391	12.994599	-0.060287	4.816035
289.703457	8000.546598	12.999603	-0.060259	4.816027
289.906990	8000.502271	13.004608	-0.060297	4.816013
290.013052	8000.588749	13.009613	-0.060317	4.816037
289.874134	8000.532773	13.014618	-0.060292	4.816022
290.252701	8000.577216	13.019623	-0.060363	4.816033
290.204023	8000.547495	13.024627	-0.060354	4.816024
290.230047	8000.529843	13.029632	-0.060360	4.816019
290.124885	8000.560036	13.034637	-0.060340	4.816028
290.080455	8000.551780	13.039642	-0.060333	4.816026
290.094024	8000.589505	13.044647	-0.060336	4.816037
289.992441	8000.473263	13.049651	-0.060317	4.816004
290.131847	8000.553939	13.054656	-0.060344	4.816026
289.951071	8000.570976	13.059661	-0.060310	4.816032
289.803898	8000.583286	13.064666	-0.060284	4.816037
290.000465	8000.530277	13.069671	-0.060321	4.816020
289.797953	8000.582203	13.074675	-0.060283	4.816036
289.887856	8000.584975	13.079680	-0.060301	4.816037
290.047336	8000.574056	13.084685	-0.060331	4.816033
289.943313	8000.533693	13.089690	-0.060312	4.816021
290.188969	8000.564996	13.094695	-0.060358	4.816029
289.903305	8000.444297	13.099699	-0.060305	4.815995
290.101830	8000.558141	13.104704	-0.060343	4.816028
290.012005	8000.547980	13.109709	-0.060327	4.816025
289.920484	8000.520679	13.114714	-0.060310	4.816018
290.097708	8000.582803	13.119719	-0.060344	4.816035
290.169875	8000.547822	13.124723	-0.060357	4.816024
290.093605	8000.512246	13.129728	-0.060344	4.816014
290.181370	8000.549198	13.134733	-0.060361	4.816025
290.118292	8000.532045	13.139738	-0.060349	4.816020
290.088730	8000.542242	13.144743	-0.060344	4.816023
290.133814	8000.558090	13.149747	-0.060353	4.816027
290.268348	8000.466512	13.154752	-0.060379	4.816000
290.154676	8000.570333	13.159757	-0.060358	4.816031
289.809714	8000.527673	13.164762	-0.060294	4.816020
290.112416	8000.593176	13.169767	-0.060351	4.816038
290.160157	8000.560953	13.174771	-0.060361	4.816028
290.178340	8000.552780	13.179776	-0.060364	4.816025
290.150141	8000.548031	13.184781	-0.060360	4.816024
290.074207	8000.535988	13.189786	-0.060346	4.816021
290.288839	8000.576345	13.194791	-0.060386	4.816032
290.212172	8000.549317	13.199795	-0.060373	4.816024
290.148080	8000.530006	13.204800	-0.060361	4.816019
290.161701	8000.560246	13.209805	-0.060364	4.816028
290.020418	8000.543791	13.214810	-0.060338	4.816024
290.149982	8000.479924	13.219815	-0.060363	4.816004
290.207079	8000.559086	13.224819	-0.060374	4.816027
290.179939	8000.543663	13.229824	-0.060370	4.816023
290.089477	8000.588028	13.234829	-0.060353	4.816036
289.805052	8000.592464	13.239834	-0.060301	4.816039
289.967710	8000.497126	13.244839	-0.060331	4.816010
289.947968	8000.598398	13.249843	-0.060328	4.816040
290.031228	8000.620296	13.254848	-0.060344	4.816046
290.270642	8000.511400	13.259853	-0.060389	4.816013
290.244213	8000.517377	13.264858	-0.060385	4.816015
290.192627	8000.614856	13.269863	-0.060376	4.816043
290.093023	8000.539285	13.274867	-0.060358	4.816022
290.100017	8000.576889	13.279872	-0.060359	4.816033
290.107935	8000.492603	13.284877	-0.060361	4.816008
290.008735	8000.578512	13.289882	-0.060343	4.816034
290.131275	8000.620381	13.294887	-0.060367	4.816045
289.931300	8000.463831	13.299891	-0.060330	4.816000
290.005852	8000.586087	13.304896	-0.060344	4.816036
290.253259	8000.588551	13.309901	-0.060391	4.816035
289.978160	8000.533275	13.314906	-0.060340	4.816020
290.177408	8000.597944	13.319911	-0.060378	4.816038
290.204618	8000.555718	13.324915	-0.060383	4.816026
290.365083	8000.473172	13.329920	-0.060414	4.816001
290.371414	8000.610214	13.334925	-0.060415	4.816041
290.263206	8000.560148	13.339930	-0.060396	4.816027
290.230531	8000.584189	13.344935	-0.060390	4.816034
290.113671	8000.573531	13.349939	-0.060369	4.816031
290.251842	8000.550458	13.354944	-0.060395	4.816024
290.462320	8000.475248	13.359949	-0.060435	4.816001
290.236389	8000.549200	13.364954	-0.060393	4.816024
290.252488	8000.612636	13.369959	-0.060397	4.816042
290.186771	8000.555867	13.374963	-0.060385	4.816026
290.251667	8000.584913	13.379968	-0.060397	4.816034
290.096185	8000.500828	13.384973	-0.060369	4.816010
290.038911	8000.599271	13.389978	-0.060359	4.816039
290.306558	8000.627772	13.394983	-0.060409	4.816046
290.198919	8000.557399	13.399987	-0.060389	4.816026
290.219816	8000.500086	13.404992	-0.060394	4.816009
290.379360	8000.568302	13.409997	-0.060424	4.816028
290.041075	8000.526833	13.415002	-0.060362	4.816018
289.971207	8000.518110	13.420007	-0.060349	4.816016
290.154070	8000.578199	13.425011	-0.060384	4.816032
290.271094	8000.556875	13.430016	-0.060406	4.816025
290.178234	8000.493191	13.435021	-0.060389	4.816007
290.029541	8000.550386	13.440026	-0.060362	4.816025
290.308897	8000.616530	13.445031	-0.060414	4.816043
290.351683	8000.585284	13.450035	-0.060423	4.816033
290.322746	8000.521707	13.455040	-0.060418	4.816015
290.469600	8000.592898	13.460045	-0.060446	4.816035
290.218191	8000.535918	13.465050	-0.060399	4.816020
290.201214	8000.588052	13.470055	-0.060397	4.816035
290.345786	8000.570443	13.475059	-0.060424	4.816029
290.414053	8000.594205	13.480064	-0.060437	4.816035
290.109696	8000.492407	13.485069	-0.060381	4.816007
290.183084	8000.550482	13.490074	-0.060395	4.816024
290.455446	8000.601526	13.495079	-0.060446	4.816037
290.154363	8000.552187	13.500083	-0.060391	4.816025
290.173909	8000.566496	13.505088	-0.060395	4.816029
290.462071	8000.564364	13.510093	-0.060449	4.816026
290.402103	8000.556891	13.515098	-0.060438	4.816025
290.483619	8000.493209	13.520103	-0.060454	4.816005
290.494897	8000.586499	13.525107	-0.060457	4.816033
290.415487	8000.557281	13.530112	-0.060442	4.816025
290.456993	8000.569856	13.535117	-0.060451	4.816028
290.280768	8000.544203	13.540122	-0.060418	4.816021
290.469566	8000.487842	13.545127	-0.060454	4.816004
290.393378	8000.555996	13.550131	-0.060440	4.816024
290.363045	8000.576872	13.555136	-0.060435	4.816030
290.274975	8000.596686	13.560141	-0.060419	4.816037
290.234774	8000.532901	13.565146	-0.060412	4.816018
290.226952	8000.574510	13.570151	-0.060411	4.816030
290.263095	8000.547420	13.575155	-0.060418	4.816022
290.342425	8000.531818	13.580160	-0.060434	4.816017
290.245946	8000.461651	13.585165	-0.060416	4.815997
290.353445	8000.534255	13.590170	-0.060437	4.816018
290.588121	8000.566427	13.595175	-0.060481	4.816026
290.423546	8000.558098	13.600179	-0.060451	4.816025
290.275037	8000.577868	13.605184	-0.060423	4.816031
290.353394	8000.600746	13.610189	-0.060439	4.816037
290.496550	8000.485799	13.615194	-0.060466	4.816003
290.286202	8000.598535	13.620199	-0.060427	4.816037
290.339852	8000.562143	13.625203	-0.060437	4.816026
290.269079	8000.572650	13.630208	-0.060425	4.816030
290.314017	8000.585289	13.635213	-0.060434	4.816033
290.095615	8000.543888	13.640218	-0.060393	4.816022
290.336660	8000.597564	13.645223	-0.060439	4.816036
290.479233	8000.529659	13.650227	-0.060466	4.816016
290.345820	8000.562539	13.655232	-0.060441	4.816026
290.469344	8000.472896	13.660237	-0.060465	4.815999
290.437769	8000.579299	13.665242	-0.060460	4.816030
290.443472	8000.589076	13.670247	-0.060461	4.816033
290.298106	8000.563990	13.675251	-0.060435	4.816027
290.378181	8000.575137	13.680256	-0.060450	4.816030
290.303932	8000.590927	13.685261	-0.060437	4.816035
290.253330	8000.594321	13.690266	-0.060428	4.816036
290.272180	8000.508097	13.695271	-0.060432	4.816010
290.190906	8000.569741	13.700275	-0.060417	4.816029
290.442618	8000.577631	13.705280	-0.060464	4.816030
290.288659	8000.597301	13.710285	-0.060436	4.816036
290.287779	8000.519269	13.715290	-0.060436	4.816014
290.327129	8000.481545	13.720295	-0.060444	4.816002
290.199600	8000.547683	13.725299	-0.060421	4.816022
290.222663	8000.597346	13.730304	-0.060426	4.816037
290.176669	8000.586923	13.735309	-0.060418	4.816034
290.231266	8000.534508	13.740314	-0.060428	4.816018
290.375676	8000.570365	13.745319	-0.060456	4.816028
290.298878	8000.550819	13.750323	-0.060442	4.816023
290.310190	8000.537174	13.755328	-0.060444	4.816019
290.414654	8000.496370	13.760333	-0.060464	4.816006
290.382593	8000.562128	13.765338	-0.060459	4.816025
290.466631	8000.593666	13.770343	-0.060475	4.816034
290.302328	8000.559677	13.775347	-0.060445	4.816025
290.531713	8000.591751	13.780352	-0.060488	4.816033
290.513599	8000.594674	13.785357	-0.060485	4.816034
290.352167	8000.556460	13.790362	-0.060456	4.816024
290.609354	8000.474625	13.795367	-0.060504	4.815999
290.493538	8000.562367	13.800371	-0.060483	4.816025
290.267636	8000.552908	13.805376	-0.060441	4.816023
290.466135	8000.576929	13.810381	-0.060479	4.816029
290.617412	8000.529502	13.815386	-0.060507	4.816015
290.457773	8000.622853	13.820391	-0.060478	4.816043
290.144288	8000.464211	13.825395	-0.060420	4.815998
290.263947	8000.558426	13.830400	-0.060443	4.816025
290.435818	8000.585164	13.835405	-0.060476	4.816032
290.316279	8000.539167	13.840410	-0.060454	4.816019
290.423617	8000.552954	13.845415	-0.060474	4.816022
290.476481	8000.561461	13.850419	-0.060485	4.816025
290.463603	8000.535607	13.855424	-0.060483	4.816017
290.510756	8000.588922	13.860429	-0.060492	4.816032
290.591490	8000.554098	13.865434	-0.060507	4.816022
290.667852	8000.518123	13.870439	-0.060522	4.816011
290.682615	8000.574050	13.875443	-0.060525	4.816027
290.522583	8000.547625	13.880448	-0.060496	4.816020
290.575814	8000.586081	13.885453	-0.060507	4.816031
290.390576	8000.605175	13.890458	-0.060473	4.816038
290.516398	8000.615025	13.895463	-0.060496	4.816040
290.454098	8000.577567	13.900467	-0.060485	4.816029
290.323444	8000.458648	13.905472	-0.060461	4.815995
290.427515	8000.612462	13.910477	-0.060481	4.816040
290.550485	8000.523878	13.915482	-0.060505	4.816013
290.691179	8000.528655	13.920487	-0.060531	4.816014
290.530069	8000.548193	13.925491	-0.060502	4.816020
290.495268	8000.588236	13.930496	-0.060496	4.816032
290.603803	8000.506871	13.935501	-0.060517	4.816008
290.443651	8000.574549	13.940506	-0.060487	4.816028
290.495419	8000.596937	13.945511	-0.060497	4.816035
290.450847	8000.576915	13.950515	-0.060490	4.816029
290.696219	8000.584690	13.955520	-0.060536	4.816030
290.552410	8000.571395	13.960525	-0.060509	4.816027
290.330011	8000.519227	13.965530	-0.060468	4.816013
290.555649	8000.603632	13.970535	-0.060511	4.816036
290.321881	8000.581196	13.975539	-0.060468	4.816031
290.613789	8000.564162	13.980544	-0.060523	4.816024
290.575324	8000.505755	13.985549	-0.060516	4.816007
290.423585	8000.572518	13.990554	-0.060488	4.816028
290.544419	8000.570513	13.995559	-0.060511	4.816026
290.582440	8000.545596	14.000563	-0.060519	4.816019
290.361022	8000.512694	14.005568	-0.060478	4.816010
290.639027	8000.575607	14.010573	-0.060530	4.816027
290.589100	8000.528752	14.015578	-0.060522	4.816014
290.820374	8000.612193	14.020583	-0.060565	4.816037
290.696549	8000.592850	14.025587	-0.060543	4.816032
290.372320	8000.494962	14.030592	-0.060483	4.816005
290.488086	8000.570928	14.035597	-0.060505	4.816027
290.480317	8000.545167	14.040602	-0.060504	4.816019
290.372618	8000.619157	14.045607	-0.060484	4.816041
290.320111	8000.560492	14.050611	-0.060475	4.816025
290.639148	8000.592080	14.055616	-0.060535	4.816032
290.511454	8000.518128	14.060621	-0.060511	4.816011
290.513669	8000.573824	14.065626	-0.060512	4.816027
290.525932	8000.602971	14.070631	-0.060515	4.816036
290.556851	8000.593963	14.075635	-0.060521	4.816033
290.462059	8000.573017	14.080640	-0.060504	4.816027
290.522030	8000.587002	14.085645	-0.060516	4.816031
290.546778	8000.439932	14.090650	-0.060521	4.815988
290.664980	8000.620742	14.095655	-0.060543	4.816040
290.732627	8000.545040	14.100659	-0.060556	4.816018
290.647262	8000.532822	14.105664	-0.060541	4.816015
290.810317	8000.578647	14.110669	-0.060572	4.816027
290.430016	8000.565276	14.115674	-0.060502	4.816025
290.630176	8000.593605	14.120679	-0.060539	4.816032
290.623196	8000.559304	14.125683	-0.060539	4.816022
290.582187	8000.606719	14.130688	-0.060531	4.816036
290.460495	8000.524323	14.135693	-0.060509	4.816013
290.484962	8000.584706	14.140698	-0.060514	4.816030
290.614380	8000.614940	14.145703	-0.060539	4.816039
290.358629	8000.548255	14.150707	-0.060492	4.816020
290.499035	8000.575484	14.155712	-0.060518	4.816028
290.507451	8000.506177	14.160717	-0.060520	4.816007
290.412409	8000.571845	14.165722	-0.060503	4.816027
290.584153	8000.604998	14.170727	-0.060536	4.816036
290.567095	8000.575859	14.175731	-0.060533	4.816027
290.586263	8000.525999	14.180736	-0.060537	4.816013
290.592893	8000.592470	14.185741	-0.060539	4.816032
290.479031	8000.503802	14.190746	-0.060518	4.816007
290.422846	8000.575532	14.195751	-0.060508	4.816028
290.270848	8000.581336	14.200755	-0.060480	4.816030
290.545564	8000.506240	14.205760	-0.060532	4.816007
290.683961	8000.613635	14.210765	-0.060558	4.816038
290.480337	8000.466637	14.215770	-0.060521	4.815996
290.491126	8000.610179	14.220775	-0.060523	4.816038
290.460329	8000.576509	14.225779	-0.060518	4.816028
290.349097	8000.611937	14.230784	-0.060498	4.816039
290.382232	8000.523837	14.235789	-0.060504	4.816013
290.381696	8000.586968	14.240794	-0.060505	4.816031
290.520848	8000.590647	14.245799	-0.060531	4.816032
290.507143	7999.408824	14.250803	-0.060528	4.815687

290.381895	7996.218238	14.255808	-0.060503	4.814756
290.564163	7990.684650	14.260813	-0.060534	4.813139
290.503623	7983.946624	14.265818	-0.060519	4.811170
290.514306	7976.672325	14.270823	-0.060517	4.809044
290.608424	7969.025950	14.275827	-0.060530	4.806807
290.431223	7961.202344	14.280832	-0.060492	4.804519
290.508200	7953.408253	14.285837	-0.060502	4.802237
290.319874	7945.350067	14.290842	-0.060462	4.799878
290.191332	7937.456720	14.295847	-0.060433	4.797566
290.047965	7929.412601	14.300851	-0.060402	4.795209
290.122086	7921.409074	14.305856	-0.060411	4.792861
290.247764	7913.398588	14.310861	-0.060430	4.790510
290.062546	7905.402940	14.315866	-0.060390	4.788163
290.007257	7897.366599	14.320871	-0.060375	4.785803
289.783588	7889.383652	14.325875	-0.060329	4.783458
289.870017	7881.433936	14.330880	-0.060340	4.781120
289.677210	7873.458343	14.335885	-0.060300	4.778775
289.834376	7865.463402	14.340890	-0.060324	4.776421
289.762684	7857.390493	14.345895	-0.060306	4.774045
289.635367	7849.371677	14.350899	-0.060278	4.771683
289.676702	7841.326510	14.355904	-0.060281	4.769311
289.578000	7833.365888	14.360909	-0.060258	4.766964
289.585345	7825.331387	14.365914	-0.060254	4.764594
289.729875	7817.436033	14.370919	-0.060277	4.762262
289.719736	7809.374330	14.375923	-0.060270	4.759882
289.647174	7801.392938	14.380928	-0.060252	4.757523
289.490664	7793.383800	14.385933	-0.060218	4.755156
289.401816	7785.324734	14.390938	-0.060196	4.752773
289.342655	7777.294396	14.395943	-0.060181	4.750397
289.122602	7769.311385	14.400947	-0.060135	4.748034
289.275105	7761.301297	14.405952	-0.060159	4.745661
289.291883	7753.386163	14.410957	-0.060157	4.743315
289.128936	7745.314863	14.415962	-0.060122	4.740922
289.031009	7737.394728	14.420967	-0.060099	4.738573
288.977517	7729.353953	14.425971	-0.060084	4.736186
289.002281	7721.320269	14.430976	-0.060084	4.733801
288.860551	7713.347564	14.435981	-0.060053	4.731432
288.890895	7705.246444	14.440986	-0.060054	4.729024
289.091154	7697.342315	14.445991	-0.060087	4.726672
288.918189	7689.341515	14.450995	-0.060050	4.724292
288.854819	7681.353323	14.456000	-0.060033	4.721914
288.872520	7673.316592	14.461005	-0.060032	4.719520
288.738123	7665.314851	14.466010	-0.060002	4.717136
288.546670	7657.349093	14.471015	-0.059962	4.714761
288.658969	7649.283700	14.476019	-0.059978	4.712355
288.700146	7641.268762	14.481024	-0.059981	4.709963
288.604345	7633.309900	14.486029	-0.059958	4.707586
288.381131	7625.294378	14.491034	-0.059912	4.705192
288.593191	7617.326645	14.496039	-0.059947	4.702809
288.426638	7609.305257	14.501043	-0.059911	4.700411
288.530507	7601.365477	14.506048	-0.059925	4.698035
288.584304	7593.322920	14.511053	-0.059931	4.695627
288.416794	7585.275352	14.516058	-0.059895	4.693216
288.191131	7577.240894	14.521063	-0.059848	4.690809
288.122028	7569.281630	14.526067	-0.059830	4.688423
288.131492	7561.247987	14.531072	-0.059827	4.686012
288.152535	7553.319433	14.536077	-0.059827	4.683633
288.001236	7545.295957	14.541082	-0.059794	4.681223
288.223150	7537.312566	14.546087	-0.059830	4.678824
287.983277	7529.325853	14.551091	-0.059781	4.676424
287.729580	7521.232215	14.556096	-0.059729	4.673990
287.760168	7513.181050	14.561101	-0.059730	4.671567
287.830372	7505.196504	14.566106	-0.059738	4.669162
287.746984	7497.201644	14.571111	-0.059718	4.666754
287.618148	7489.220000	14.576115	-0.059689	4.664349
287.528790	7481.246898	14.581120	-0.059668	4.661944
287.597462	7473.220895	14.586125	-0.059676	4.659523
287.445861	7465.246465	14.591130	-0.059643	4.657116
287.566783	7457.232156	14.596135	-0.059661	4.654695
287.380815	7449.233887	14.601139	-0.059621	4.652278
287.383783	7441.214943	14.606144	-0.059617	4.649853
287.612863	7433.272410	14.611149	-0.059655	4.647450
287.133398	7425.183349	14.616154	-0.059561	4.645003
287.276672	7417.265217	14.621159	-0.059583	4.642605
287.418548	7409.245017	14.626163	-0.059605	4.640175
287.374877	7401.272544	14.631168	-0.059592	4.637758
287.249158	7393.223690	14.636173	-0.059564	4.635317
287.088817	7385.179016	14.641178	-0.059529	4.632876
287.249757	7377.191075	14.646183	-0.059554	4.630450
287.197115	7369.199433	14.651187	-0.059540	4.628023
287.003955	7361.167463	14.656192	-0.059499	4.625581
287.200393	7353.232175	14.661197	-0.059531	4.623168
287.037958	7345.171871	14.666202	-0.059496	4.620716
287.038410	7337.228031	14.671207	-0.059491	4.618297
286.960976	7329.193927	14.676211	-0.059472	4.615850
286.946247	7321.178574	14.681216	-0.059465	4.613408
286.819376	7313.167298	14.686221	-0.059436	4.610965
286.630578	7305.131589	14.691226	-0.059396	4.608514
286.627584	7297.161818	14.696231	-0.059391	4.606081
286.635158	7289.166639	14.701235	-0.059388	4.603639
286.516675	7281.183772	14.706240	-0.059361	4.601200
286.446467	7273.203182	14.711245	-0.059343	4.598760
286.411628	7265.140146	14.716250	-0.059332	4.596294
286.350169	7257.115107	14.721255	-0.059316	4.593838
286.343569	7249.090318	14.726259	-0.059310	4.591380
286.324411	7241.150315	14.731264	-0.059302	4.588948
286.284974	7233.120872	14.736269	-0.059290	4.586486
286.083833	7225.093813	14.741274	-0.059247	4.584024
286.220539	7217.158375	14.746279	-0.059268	4.581589
286.333459	7209.132595	14.751283	-0.059284	4.579125
286.138559	7201.156146	14.756288	-0.059243	4.576675
285.990278	7193.146420	14.761293	-0.059211	4.574213
286.075972	7185.084900	14.766298	-0.059222	4.571733
286.076310	7177.121192	14.771303	-0.059218	4.569283
285.983524	7169.086919	14.776307	-0.059196	4.566809
285.996160	7161.112550	14.781312	-0.059193	4.564353
285.829851	7153.171242	14.786317	-0.059158	4.561905
285.609942	7145.079544	14.791322	-0.059112	4.559410
285.708074	7137.206985	14.796327	-0.059125	4.556981
285.631733	7129.107564	14.801331	-0.059106	4.554481
285.585141	7121.086303	14.806336	-0.059093	4.552003
285.781212	7113.083791	14.811341	-0.059125	4.549530
285.737304	7105.111627	14.816346	-0.059112	4.547065
285.673574	7097.084361	14.821351	-0.059095	4.544581
285.462181	7089.119557	14.826355	-0.059051	4.542116
285.673407	7081.090948	14.831360	-0.059086	4.539629
285.551977	7073.193970	14.836365	-0.059058	4.537182
285.468662	7065.088740	14.841370	-0.059038	4.534669
285.344331	7057.167314	14.846375	-0.059010	4.532211
285.212250	7049.087384	14.851379	-0.058981	4.529703
284.975419	7041.115021	14.856384	-0.058932	4.527226
285.083577	7033.080033	14.861389	-0.058948	4.524730
284.917901	7025.122202	14.866394	-0.058912	4.522255
285.000162	7017.076107	14.871399	-0.058923	4.519752
284.679970	7009.185187	14.876403	-0.058858	4.517296
284.679327	7001.060259	14.881408	-0.058853	4.514765
284.732622	6993.048735	14.886413	-0.058859	4.512269
284.556453	6985.005059	14.891418	-0.058821	4.509761
284.750539	6977.075551	14.896423	-0.058852	4.507287
284.688761	6969.052066	14.901427	-0.058836	4.504783
284.689110	6961.107597	14.906432	-0.058832	4.502302
284.633193	6953.086012	14.911437	-0.058816	4.499795
284.535657	6945.099182	14.916442	-0.058793	4.497298
284.729406	6937.048780	14.921447	-0.058825	4.494780
284.558042	6929.084430	14.926451	-0.058788	4.492287
284.662090	6920.988839	14.931456	-0.058803	4.489752
284.591741	6913.093439	14.936461	-0.058785	4.487278
284.287569	6904.974420	14.941466	-0.058724	4.484731
284.317034	6897.087118	14.946471	-0.058724	4.482257
284.239836	6889.038043	14.951475	-0.058705	4.479730
284.217262	6881.108342	14.956480	-0.058696	4.477240
284.243949	6873.079320	14.961485	-0.058697	4.474717
284.256667	6865.029143	14.966490	-0.058694	4.472186
284.256125	6857.032266	14.971495	-0.058689	4.469670
284.241361	6849.042021	14.976499	-0.058682	4.467155
284.193032	6840.978332	14.981504	-0.058668	4.464616
284.046129	6833.068821	14.986509	-0.058636	4.462123
283.852194	6825.003918	14.991514	-0.058595	4.459579
283.991522	6817.052984	14.996519	-0.058616	4.457071
283.922885	6809.012791	15.001523	-0.058599	4.454533
283.871689	6800.989872	15.006528	-0.058585	4.451999
283.906116	6793.002204	15.011533	-0.058586	4.449475
283.531190	6785.000978	15.016538	-0.058512	4.446944
283.702994	6777.022851	15.021543	-0.058539	4.444420
283.536477	6769.065961	15.026547	-0.058503	4.441901
283.608390	6761.027072	15.031552	-0.058512	4.439355
283.736854	6753.051179	15.036557	-0.058531	4.436827
283.513605	6745.023076	15.041562	-0.058485	4.434281
283.497968	6736.975454	15.046567	-0.058477	4.431727
283.318058	6728.982734	15.051571	-0.058439	4.429189
283.358972	6720.945659	15.056576	-0.058442	4.426636
283.207427	6713.000170	15.061581	-0.058409	4.424110
283.244863	6705.013604	15.066586	-0.058411	4.421570
283.219757	6697.021669	15.071591	-0.058402	4.419027
283.134093	6688.973420	15.076595	-0.058381	4.416464
283.141919	6680.951125	15.081600	-0.058378	4.413909
283.076028	6672.987387	15.086605	-0.058361	4.411370
282.902338	6664.969129	15.091610	-0.058324	4.408812
282.988707	6656.984127	15.096615	-0.058335	4.406264
282.831924	6648.985764	15.101619	-0.058301	4.403709
282.927051	6640.968847	15.106624	-0.058314	4.401148
282.770894	6632.993528	15.111629	-0.058280	4.398598
282.661494	6624.983164	15.116634	-0.058255	4.396035
282.787312	6616.984630	15.121639	-0.058274	4.393475
282.607260	6608.965268	15.126643	-0.058236	4.390906
282.572901	6600.952277	15.131648	-0.058225	4.388339
282.606691	6592.914678	15.136653	-0.058226	4.385762
282.559180	6584.976506	15.141658	-0.058213	4.383215
282.535989	6577.013406	15.146663	-0.058203	4.380658
282.446050	6569.041501	15.151667	-0.058182	4.378097
282.404870	6560.963747	15.156672	-0.058170	4.375501
282.317650	6552.993501	15.161677	-0.058149	4.372938
282.101947	6544.942875	15.166682	-0.058104	4.370346
282.177796	6537.014208	15.171687	-0.058113	4.367794
282.172803	6528.956899	15.176691	-0.058107	4.365198
282.054235	6520.998392	15.181696	-0.058081	4.362632
282.168749	6513.003671	15.186701	-0.058097	4.360054
281.997103	6505.022693	15.191706	-0.058061	4.357478
282.022432	6496.984911	15.196711	-0.058061	4.354883
282.041132	6488.857375	15.201715	-0.058059	4.352257
281.959108	6480.862129	15.206720	-0.058039	4.349671
281.970554	6472.973144	15.211725	-0.058037	4.347119
281.908186	6464.893498	15.216730	-0.058020	4.344504
282.146472	6456.993154	15.221735	-0.058060	4.341947
281.927574	6448.919446	15.226739	-0.058014	4.339329
281.728548	6441.013940	15.231744	-0.057973	4.336764
281.644122	6432.979134	15.236749	-0.057952	4.334156
281.650331	6424.939695	15.241754	-0.057949	4.331546
281.537124	6416.931545	15.246759	-0.057923	4.328944
281.634489	6408.941237	15.251763	-0.057936	4.326348
281.493231	6400.930877	15.256768	-0.057905	4.323741
281.480343	6393.003291	15.261773	-0.057898	4.321161
281.307210	6384.945808	15.266778	-0.057861	4.318536
281.416015	6376.950530	15.271783	-0.057877	4.315932
281.380860	6368.940153	15.276787	-0.057865	4.313320
281.128035	6360.903962	15.281792	-0.057814	4.310697
281.142993	6352.954887	15.286797	-0.057812	4.308102
281.188167	6344.913428	15.291802	-0.057815	4.305476
281.246610	6336.928136	15.296807	-0.057821	4.302867
281.213292	6328.946866	15.301811	-0.057811	4.300256
281.110570	6320.907174	15.306816	-0.057787	4.297625
281.139211	6312.940949	15.311821	-0.057787	4.295017
280.996408	6304.930155	15.316826	-0.057756	4.292391
281.052458	6296.910194	15.321831	-0.057762	4.289762
280.884005	6288.937492	15.326835	-0.057726	4.287146
280.707797	6280.905257	15.331840	-0.057688	4.284508
280.997539	6272.943935	15.336845	-0.057737	4.281895
280.806919	6264.904862	15.341850	-0.057697	4.279252
280.811482	6256.939203	15.346855	-0.057693	4.276633
280.538891	6248.929221	15.351859	-0.057638	4.273995
280.597162	6240.850766	15.356864	-0.057644	4.271336
280.609261	6232.902570	15.361869	-0.057641	4.268717
280.501115	6224.870419	15.366874	-0.057616	4.266068
280.390448	6216.907709	15.371879	-0.057591	4.263441
280.516858	6208.867358	15.376883	-0.057610	4.260788
280.454647	6200.907663	15.381888	-0.057594	4.258159
280.367935	6192.919548	15.386893	-0.057573	4.255518
280.087449	6184.882000	15.391898	-0.057516	4.252858
280.079678	6176.884919	15.396903	-0.057510	4.250212
280.181959	6168.867309	15.401907	-0.057524	4.247558
280.023321	6160.897392	15.406912	-0.057490	4.244916
280.016190	6152.941640	15.411917	-0.057484	4.242279
279.901514	6144.859197	15.416922	-0.057457	4.239597
279.969964	6136.964071	15.421927	-0.057465	4.236977
279.964207	6128.922665	15.426931	-0.057460	4.234306
279.710331	6120.864993	15.431936	-0.057408	4.231626
279.776771	6112.922852	15.436941	-0.057415	4.228985
279.726364	6104.891370	15.441946	-0.057401	4.226312
279.908659	6096.917510	15.446951	-0.057430	4.223659
279.592624	6088.924282	15.451955	-0.057367	4.220992
279.522405	6080.939537	15.456960	-0.057349	4.218330
279.818854	6072.948421	15.461965	-0.057399	4.215666
279.717555	6064.906407	15.466970	-0.057376	4.212981
279.672956	6056.914637	15.471975	-0.057363	4.210311
279.592339	6048.914076	15.476979	-0.057343	4.207636
279.567257	6040.900210	15.481984	-0.057334	4.204956
279.564812	6032.968202	15.486989	-0.057329	4.202301
279.587730	6024.945397	15.491994	-0.057328	4.199614
279.439384	6017.006445	15.496999	-0.057296	4.196953
279.142019	6008.903981	15.502003	-0.057236	4.194233
279.230926	6000.770033	15.507008	-0.057247	4.191504
279.275449	5992.839775	15.512013	-0.057251	4.188842
279.132221	5984.883175	15.517018	-0.057220	4.186168
279.145749	5976.878589	15.522023	-0.057217	4.183477
279.057507	5968.893463	15.527027	-0.057196	4.180790
278.852488	5960.926454	15.532032	-0.057153	4.178106
278.909363	5952.910050	15.537037	-0.057159	4.175406
278.739860	5944.900456	15.542042	-0.057123	4.172705
278.820508	5936.858512	15.547047	-0.057133	4.169993
278.797663	5928.916653	15.552051	-0.057124	4.167313
278.678879	5920.892460	15.557056	-0.057097	4.164601
278.704322	5912.949198	15.562061	-0.057097	4.161917
278.624270	5904.869611	15.567066	-0.057078	4.159184
278.717981	5896.950132	15.572071	-0.057090	4.156506
278.655919	5888.887883	15.577075	-0.057074	4.153775
278.470889	5880.853492	15.582080	-0.057035	4.151051
278.342255	5872.926587	15.587085	-0.057006	4.148362
278.395733	5864.855225	15.592090	-0.057011	4.145624
278.363932	5856.927214	15.597095	-0.057001	4.142933
278.302059	5848.893318	15.602099	-0.056985	4.140203
278.101009	5840.892485	15.607104	-0.056942	4.137481
278.236817	5832.891797	15.612109	-0.056963	4.134761
278.039966	5824.866616	15.617114	-0.056922	4.132027
278.003519	5816.851312	15.622119	-0.056910	4.129296
277.991788	5808.899982	15.627123	-0.056903	4.126586
277.927257	5800.884376	15.632128	-0.056886	4.123852
278.050957	5792.870179	15.637133	-0.056905	4.121118
277.918758	5784.928879	15.642138	-0.056875	4.118404
278.054535	5776.922066	15.647143	-0.056896	4.115670
277.808455	5768.882287	15.652147	-0.056845	4.112917
277.663713	5760.819696	15.657152	-0.056814	4.110157
277.709350	5752.877773	15.662157	-0.056817	4.107438
277.652384	5744.826454	15.667162	-0.056802	4.104678
277.509804	5736.909344	15.672167	-0.056771	4.101962
277.524777	5728.866180	15.677171	-0.056769	4.099202
277.402511	5720.878995	15.682176	-0.056741	4.096458
277.344700	5712.919330	15.687181	-0.056726	4.093723
277.293405	5704.842225	15.692186	-0.056712	4.090945
277.605455	5696.877527	15.697191	-0.056765	4.088209
277.405833	5688.880396	15.702195	-0.056723	4.085453
277.288251	5680.924567	15.707200	-0.056696	4.082711
277.257374	5672.934594	15.712205	-0.056686	4.079956
277.113677	5664.939920	15.717210	-0.056655	4.077196
276.906715	5656.944142	15.722215	-0.056611	4.074433
277.154650	5648.899086	15.727219	-0.056653	4.071657
277.053959	5640.892955	15.732224	-0.056629	4.068888
276.909977	5632.934628	15.737229	-0.056598	4.066133
276.809097	5624.915139	15.742234	-0.056574	4.063356
276.855098	5616.914254	15.747239	-0.056578	4.060585
276.744777	5608.964688	15.752243	-0.056553	4.057828
276.707117	5600.943876	15.757248	-0.056541	4.055046
276.902801	5592.924561	15.762253	-0.056573	4.052265
276.765322	5584.890054	15.767258	-0.056542	4.049472
276.763008	5576.958001	15.772263	-0.056537	4.046715
276.552263	5568.950174	15.777267	-0.056493	4.043927
276.676618	5560.920717	15.782272	-0.056512	4.041134
276.665820	5552.965079	15.787277	-0.056505	4.038363
276.395907	5544.908383	15.792282	-0.056450	4.035551
276.429541	5536.833115	15.797287	-0.056451	4.032735
276.307776	5528.814707	15.802291	-0.056424	4.029934
276.289779	5520.894952	15.807296	-0.056416	4.027168
276.422882	5512.888533	15.812301	-0.056436	4.024372
276.266310	5504.912445	15.817306	-0.056402	4.021580
276.446223	5496.907971	15.822311	-0.056431	4.018781
276.357912	5488.912499	15.827315	-0.056410	4.015979
276.150198	5480.914444	15.832320	-0.056366	4.013173
276.118669	5472.878852	15.837325	-0.056356	4.010354
276.043423	5464.900626	15.842330	-0.056337	4.007553
276.010095	5456.914632	15.847335	-0.056326	4.004747
275.852755	5448.970777	15.852339	-0.056292	4.001953
275.794976	5440.904818	15.857344	-0.056277	3.999115
275.757848	5432.949213	15.862349	-0.056265	3.996314
275.698380	5424.886788	15.867354	-0.056249	3.993473
275.645496	5416.882076	15.872359	-0.056234	3.990651
275.633493	5408.911302	15.877363	-0.056228	3.987839
275.760881	5400.876219	15.882368	-0.056246	3.985005
275.590979	5392.958335	15.887373	-0.056210	3.982206
275.286883	5384.922413	15.892378	-0.056149	3.979360
275.216907	5376.965496	15.897383	-0.056131	3.976544
275.378365	5368.926935	15.902387	-0.056156	3.973702
275.133856	5360.880165	15.907392	-0.056106	3.970847
275.142458	5352.942912	15.912397	-0.056103	3.968034
275.025238	5344.891332	15.917402	-0.056076	3.965175
275.043730	5336.972907	15.922407	-0.056075	3.962365
274.901006	5328.962233	15.927411	-0.056044	3.959516
274.994394	5320.977886	15.932416	-0.056057	3.956679
275.055634	5312.986715	15.937421	-0.056063	3.953838
274.877427	5304.926721	15.942426	-0.056025	3.950965
274.974414	5296.932268	15.947431	-0.056039	3.948118
274.976998	5288.933180	15.952435	-0.056034	3.945266
274.885284	5280.944408	15.957440	-0.056013	3.942414
274.850601	5272.963957	15.962445	-0.056001	3.939564
274.912254	5264.982019	15.967450	-0.056008	3.936713
274.844399	5256.995553	15.972455	-0.055991	3.933856
274.469250	5248.953170	15.977459	-0.055916	3.930972
274.561423	5240.971526	15.982464	-0.055929	3.928115
274.763091	5232.964145	15.987469	-0.055961	3.925249
274.516970	5224.981160	15.992474	-0.055911	3.922382
274.453489	5216.995070	15.997479	-0.055894	3.919515
274.477578	5209.027009	16.002483	-0.055894	3.916654
274.224869	5201.010000	16.007488	-0.055842	3.913768
274.190406	5192.974189	16.012493	-0.055831	3.910877
274.245099	5184.945053	16.017498	-0.055837	3.907987
274.260176	5176.961961	16.022503	-0.055835	3.905112
273.997922	5169.007477	16.027507	-0.055781	3.902240
273.880868	5160.983230	16.032512	-0.055755	3.899343
274.023002	5153.031277	16.037517	-0.055776	3.896475
273.877585	5144.989318	16.042522	-0.055745	3.893567
273.800334	5136.977544	16.047527	-0.055725	3.890668
273.774366	5128.984651	16.052531	-0.055716	3.887776
273.738334	5120.948259	16.057536	-0.055704	3.884865
273.784918	5113.035037	16.062541	-0.055708	3.881999
273.875030	5104.991118	16.067546	-0.055720	3.879083
273.920151	5097.009752	16.072551	-0.055724	3.876188
273.720185	5088.856491	16.077555	-0.055682	3.873223
273.511322	5080.797616	16.082560	-0.055638	3.870290
273.561897	5072.904482	16.087565	-0.055643	3.867420
273.333000	5064.895768	16.092570	-0.055596	3.864500
273.303753	5056.963917	16.097575	-0.055586	3.861610
273.243364	5048.992611	16.102579	-0.055570	3.858703
273.271193	5040.981535	16.107584	-0.055570	3.855780
273.202060	5032.978348	16.112589	-0.055552	3.852857
273.127646	5024.934583	16.117594	-0.055534	3.849916
273.033500	5016.989393	16.122599	-0.055512	3.847009
273.044302	5009.000176	16.127603	-0.055509	3.844086
273.024918	5001.034883	16.132608	-0.055501	3.841168
273.310008	4993.025690	16.137613	-0.055549	3.838239
273.047314	4985.032331	16.142618	-0.055495	3.835301
272.973561	4977.016887	16.147623	-0.055477	3.832358
272.867638	4969.000935	16.152627	-0.055452	3.829411
272.597890	4961.031757	16.157632	-0.055397	3.826475
272.590722	4953.064286	16.162637	-0.055391	3.823544
272.743541	4945.031223	16.167642	-0.055415	3.820589
272.685220	4937.075506	16.172647	-0.055400	3.817656
272.589414	4929.073048	16.177651	-0.055377	3.814703
272.631702	4921.047852	16.182656	-0.055380	3.811742
272.633944	4913.048904	16.187661	-0.055376	3.808788
272.336630	4905.058945	16.192666	-0.055316	3.805828
272.360877	4897.098222	16.197671	-0.055316	3.802884
272.443329	4889.072028	16.202675	-0.055326	3.799914
272.500868	4881.090579	16.207680	-0.055332	3.796958
272.539950	4873.105453	16.212685	-0.055335	3.793998
272.329648	4865.046022	16.217690	-0.055291	3.791003
272.457474	4857.087609	16.222695	-0.055310	3.788050
272.342068	4849.063947	16.227699	-0.055284	3.785066
272.194196	4841.094721	16.232704	-0.055251	3.782098
272.262718	4833.103976	16.237709	-0.055259	3.779125
271.907027	4825.108561	16.242714	-0.055188	3.776139
271.894518	4817.087553	16.247719	-0.055181	3.773148
271.841084	4809.067824	16.252723	-0.055167	3.770154
271.811496	4801.053906	16.257728	-0.055156	3.767161
271.938924	4793.097088	16.262733	-0.055175	3.764190
271.642577	4785.107732	16.267738	-0.055116	3.761195
271.623785	4777.108136	16.272743	-0.055107	3.758200
271.572402	4769.123565	16.277747	-0.055093	3.755208
271.703422	4761.053579	16.282752	-0.055113	3.752185
271.838127	4753.098768	16.287757	-0.055133	3.749203
271.640083	4745.070007	16.292762	-0.055091	3.746183
271.389405	4737.139054	16.297767	-0.055040	3.743197
271.404642	4729.117718	16.302771	-0.055038	3.740180
271.532353	4721.124931	16.307776	-0.055057	3.737174
271.588831	4713.132163	16.312781	-0.055063	3.734164
271.379204	4705.104400	16.317786	-0.055019	3.731133
271.467789	4697.130024	16.322791	-0.055031	3.728125
271.281161	4689.132963	16.327795	-0.054992	3.725101
271.300886	4681.161757	16.332800	-0.054990	3.722088
271.267312	4673.164051	16.337805	-0.054979	3.719062
271.184847	4665.189970	16.342810	-0.054959	3.716041
270.843511	4657.142423	16.347815	-0.054891	3.712984
270.912081	4649.078127	16.352819	-0.054899	3.709928
270.902819	4641.095296	16.357824	-0.054893	3.706898
270.738924	4633.137908	16.362829	-0.054857	3.703871
270.788408	4625.144709	16.367834	-0.054862	3.700834
270.954262	4617.189955	16.372839	-0.054888	3.697811
270.903284	4609.164630	16.377843	-0.054874	3.694754
270.651346	4601.189256	16.382848	-0.054822	3.691709
270.777967	4593.193596	16.387853	-0.054841	3.688662
270.585425	4585.164737	16.392858	-0.054800	3.685593
270.316144	4577.257117	16.397863	-0.054746	3.682565
270.286595	4569.231900	16.402867	-0.054735	3.679496
270.411574	4561.263609	16.407872	-0.054754	3.676450
270.494935	4553.217425	16.412877	-0.054765	3.673370
270.158901	4545.204810	16.417882	-0.054697	3.670290
270.436545	4537.219479	16.422887	-0.054744	3.667234
270.409609	4529.204005	16.427891	-0.054735	3.664156
270.281202	4521.234521	16.432896	-0.054706	3.661090
270.308216	4513.254097	16.437901	-0.054706	3.658021
270.332734	4505.208378	16.442906	-0.054706	3.654925
270.314940	4497.237922	16.447911	-0.054698	3.651854
270.316526	4489.217036	16.452915	-0.054694	3.648761
270.257648	4481.225636	16.457920	-0.054678	3.645676
270.261250	4473.265080	16.462925	-0.054674	3.642601
269.907162	4465.275804	16.467930	-0.054603	3.639503
270.113279	4457.306956	16.472935	-0.054637	3.636426
269.970296	4449.265460	16.477939	-0.054606	3.633308
269.755293	4441.231843	16.482944	-0.054561	3.630189
269.656793	4433.288137	16.487949	-0.054538	3.627105
269.562420	4425.265748	16.492954	-0.054515	3.623988
269.683008	4417.279627	16.497959	-0.054533	3.620888
269.410436	4409.309081	16.502963	-0.054478	3.617781
269.513188	4401.284154	16.507968	-0.054492	3.614660
269.492187	4393.301975	16.512973	-0.054483	3.611550
269.385674	4385.282239	16.517978	-0.054459	3.608420
269.565427	4377.308630	16.522983	-0.054488	3.605314
269.306449	4369.368649	16.527987	-0.054435	3.602205
269.123649	4361.356036	16.532992	-0.054396	3.599068
269.256301	4353.388825	16.537997	-0.054416	3.595955
269.319936	4345.349676	16.543002	-0.054423	3.592808
269.089186	4337.331294	16.548007	-0.054375	3.589659
269.053301	4329.365041	16.553011	-0.054364	3.586533
269.105039	4321.371678	16.558016	-0.054369	3.583396
269.182612	4313.385033	16.563021	-0.054379	3.580260
268.806720	4305.397462	16.568026	-0.054304	3.577107
268.908228	4297.398580	16.573031	-0.054318	3.573961
268.844130	4289.379060	16.578035	-0.054301	3.570800
268.723359	4281.391352	16.583040	-0.054274	3.567646
268.703962	4273.377318	16.588045	-0.054266	3.564482
268.765568	4265.416647	16.593050	-0.054273	3.561339
268.923148	4257.437824	16.598055	-0.054297	3.558189
268.832102	4249.430581	16.603059	-0.054276	3.555017
268.697541	4241.310831	16.608064	-0.054246	3.551797
268.786293	4233.356019	16.613069	-0.054257	3.548645
268.669464	4225.357349	16.618074	-0.054231	3.545468
268.698860	4217.414801	16.623079	-0.054232	3.542314
268.713436	4209.417622	16.628083	-0.054230	3.539135
268.462945	4201.418318	16.633088	-0.054178	3.535945
268.345606	4193.445416	16.638093	-0.054152	3.532766
268.216163	4185.397675	16.643098	-0.054123	3.529554
268.343811	4177.415483	16.648103	-0.054142	3.526373
268.279126	4169.443952	16.653107	-0.054125	3.523188
268.087667	4161.465014	16.658112	-0.054085	3.519992
268.020651	4153.530811	16.663117	-0.054068	3.516816
268.001485	4145.473168	16.668122	-0.054059	3.513589
267.972415	4137.461063	16.673127	-0.054049	3.510377
267.946215	4129.466981	16.678131	-0.054040	3.507169
268.067737	4121.461185	16.683136	-0.054058	3.503958
267.926898	4113.510698	16.688141	-0.054027	3.500758
267.752456	4105.535221	16.693146	-0.053989	3.497544
267.750991	4097.525183	16.698151	-0.053984	3.494319
267.674004	4089.543079	16.703155	-0.053965	3.491100
267.548015	4081.526525	16.708160	-0.053937	3.487862
267.480355	4073.551599	16.713165	-0.053920	3.484640
267.433626	4065.607167	16.718170	-0.053906	3.481427
267.493852	4057.591568	16.723175	-0.053913	3.478187
267.350314	4049.603946	16.728179	-0.053881	3.474948
267.199278	4041.542815	16.733184	-0.053849	3.471676
267.262686	4033.568684	16.738189	-0.053856	3.468443
267.066504	4025.569354	16.743194	-0.053814	3.465189
267.304758	4017.587911	16.748199	-0.053854	3.461953
267.285148	4009.597388	16.753203	-0.053846	3.458701
267.211912	4001.584155	16.758208	-0.053827	3.455436
267.094986	3993.620285	16.763213	-0.053801	3.452186
267.057746	3985.607146	16.768218	-0.053789	3.448916
266.962346	3977.608563	16.773223	-0.053767	3.445647
267.002409	3969.664801	16.778227	-0.053769	3.442401
267.027278	3961.623719	16.783232	-0.053769	3.439112
267.009359	3953.689009	16.788237	-0.053761	3.435862
266.764824	3945.679598	16.793242	-0.053711	3.432571
266.787456	3937.648797	16.798247	-0.053710	3.429276
266.504336	3929.660347	16.803251	-0.053653	3.425986
266.411798	3921.690042	16.808256	-0.053631	3.422706
266.546511	3913.695279	16.813261	-0.053651	3.419421
266.390057	3905.715226	16.818266	-0.053618	3.416129
266.260467	3897.694578	16.823271	-0.053589	3.412818
266.095101	3889.715712	16.828275	-0.053553	3.409519
266.181284	3881.716427	16.833280	-0.053565	3.406218
266.267215	3873.744503	16.838285	-0.053576	3.402925
266.052839	3865.756045	16.843290	-0.053531	3.399611
266.058442	3857.800209	16.848295	-0.053527	3.396315
266.245548	3849.724177	16.853299	-0.053558	3.392972
266.043259	3841.665841	16.858304	-0.053515	3.389620
266.177671	3833.734705	16.863309	-0.053535	3.386329
266.060518	3825.738453	16.868314	-0.053509	3.382999
265.962733	3817.755257	16.873319	-0.053486	3.379672
265.916192	3809.816852	16.878323	-0.053473	3.376362
265.759325	3801.805029	16.883328	-0.053439	3.373015
265.827231	3793.788265	16.888333	-0.053447	3.369669
265.527580	3785.837367	16.893338	-0.053386	3.366335
265.627255	3777.853212	16.898343	-0.053400	3.362998
265.622056	3769.839650	16.903347	-0.053394	3.359642
265.282309	3761.907223	16.908352	-0.053326	3.356304
265.418637	3753.877564	16.913357	-0.053347	3.352939
265.398855	3745.823938	16.918362	-0.053338	3.349555
265.330804	3737.863481	16.923367	-0.053321	3.346205
265.379661	3729.862445	16.928371	-0.053325	3.342839
265.300986	3721.875981	16.933376	-0.053306	3.339471
265.215699	3713.944791	16.938381	-0.053286	3.336123
265.166552	3705.875109	16.943386	-0.053272	3.332714
265.334326	3697.858407	16.948391	-0.053298	3.329332
264.968906	3689.925579	16.953395	-0.053225	3.325962
264.927955	3681.946940	16.958400	-0.053213	3.322582
265.098805	3673.971953	16.963405	-0.053240	3.319207
264.930511	3665.976559	16.968410	-0.053204	3.315808
264.948906	3657.958400	16.973415	-0.053203	3.312402
264.859244	3649.944763	16.978419	-0.053181	3.308991
264.868154	3641.949818	16.983424	-0.053178	3.305588
264.768153	3634.023236	16.988429	-0.053155	3.302207
264.763882	3625.991757	16.993434	-0.053149	3.298781
264.554198	3618.047477	16.998439	-0.053106	3.295381
264.486924	3610.044837	17.003443	-0.053088	3.291957
264.489124	3602.005726	17.008448	-0.053084	3.288517
264.521210	3594.035739	17.013453	-0.053085	3.285105
264.404478	3586.069128	17.018458	-0.053059	3.281684
264.303196	3578.104411	17.023463	-0.053035	3.278262
264.288351	3570.114888	17.028467	-0.053028	3.274828
264.384028	3562.067955	17.033472	-0.053041	3.271371
264.381054	3554.084758	17.038477	-0.053036	3.267933
264.027538	3546.096755	17.043482	-0.052965	3.264476
264.217992	3538.141892	17.048487	-0.052996	3.261051
264.107447	3530.136650	17.053491	-0.052970	3.257588
263.957996	3522.116815	17.058496	-0.052938	3.254115
263.865644	3514.130690	17.063501	-0.052916	3.250654
263.773252	3506.156001	17.068506	-0.052894	3.247194
263.721360	3498.174643	17.073511	-0.052880	3.243730
263.855617	3490.175427	17.078515	-0.052900	3.240261
263.765194	3482.229766	17.083520	-0.052878	3.236803
263.887647	3474.189870	17.088525	-0.052896	3.233309
263.594305	3466.150434	17.093530	-0.052837	3.229795
263.651229	3458.194806	17.098535	-0.052843	3.226327
263.550719	3450.211560	17.103539	-0.052820	3.222837
263.238378	3442.225993	17.108544	-0.052757	3.219334
263.395970	3434.273986	17.113549	-0.052781	3.215861
263.466582	3426.262394	17.118554	-0.052790	3.212354
263.243116	3418.266371	17.123559	-0.052743	3.208839
263.009030	3410.288036	17.128563	-0.052695	3.205326
263.055802	3402.306402	17.133568	-0.052699	3.201820
263.163606	3394.327749	17.138573	-0.052714	3.198314
262.982197	3386.314213	17.143578	-0.052676	3.194777
262.817796	3378.358985	17.148583	-0.052641	3.191262
262.849620	3370.351625	17.153587	-0.052642	3.187729
262.691315	3362.346450	17.158592	-0.052608	3.184185
262.830384	3354.394649	17.163597	-0.052629	3.180672
262.707206	3346.398342	17.168602	-0.052601	3.177125
262.834221	3338.394895	17.173607	-0.052620	3.173582
262.775677	3330.382924	17.178611	-0.052604	3.170023
262.637092	3322.424860	17.183616	-0.052574	3.166480
262.778707	3314.411705	17.188621	-0.052596	3.162921
262.584975	3306.446065	17.193626	-0.052555	3.159365
262.681865	3298.486668	17.198631	-0.052568	3.155820
262.551425	3290.461673	17.203635	-0.052539	3.152232
262.297273	3282.482988	17.208640	-0.052487	3.148655
262.122978	3274.495295	17.213645	-0.052450	3.145073
262.015597	3266.536755	17.218650	-0.052425	3.141504
262.188975	3258.527976	17.223655	-0.052453	3.137920
262.148707	3250.541461	17.228659	-0.052440	3.134332
261.886648	3242.553863	17.233664	-0.052387	3.130730
261.881055	3234.570576	17.238669	-0.052381	3.127137
261.766173	3226.576723	17.243674	-0.052355	3.123531
261.739591	3218.602155	17.248679	-0.052345	3.119933
261.987693	3210.629082	17.253683	-0.052387	3.116343
261.847666	3202.596419	17.258688	-0.052356	3.112706
261.842262	3194.619184	17.263693	-0.052350	3.109095
261.653053	3186.633635	17.268698	-0.052310	3.105468
261.691791	3178.656882	17.273703	-0.052313	3.101850
261.782726	3170.677353	17.278707	-0.052325	3.098230
261.641821	3162.693170	17.283712	-0.052294	3.094593
261.682781	3154.680405	17.288717	-0.052297	3.090947
261.474141	3146.715063	17.293722	-0.052253	3.087307
261.381748	3138.740729	17.298727	-0.052232	3.083663
261.357783	3130.751919	17.303731	-0.052222	3.080012
261.318422	3122.805521	17.308736	-0.052210	3.076375
261.323444	3114.768689	17.313741	-0.052207	3.072695
261.228674	3106.725033	17.318746	-0.052184	3.069002
261.268443	3098.745445	17.323751	-0.052187	3.065340
261.178392	3090.798047	17.328755	-0.052165	3.061683
261.157410	3082.802999	17.333760	-0.052157	3.058003
261.204610	3074.818770	17.338765	-0.052161	3.054327
260.973161	3066.827925	17.343770	-0.052113	3.050630
260.829835	3058.869627	17.348775	-0.052082	3.046947
261.023039	3050.870361	17.353779	-0.052113	3.043257
260.992174	3042.884150	17.358784	-0.052102	3.039558
260.987543	3034.955460	17.363789	-0.052097	3.035883
260.736630	3026.949480	17.368794	-0.052045	3.032155
260.612087	3018.946476	17.373799	-0.052017	3.028430
260.670478	3010.968668	17.378803	-0.052024	3.024721
260.704981	3002.974289	17.383808	-0.052025	3.020999
260.633442	2995.014801	17.388813	-0.052007	3.017283
260.375707	2987.041759	17.393818	-0.051955	3.013547
260.244980	2979.031474	17.398823	-0.051925	3.009796
260.279394	2971.062659	17.403827	-0.051927	3.006067
260.313782	2963.071101	17.408832	-0.051929	3.002323
260.210262	2955.117240	17.413837	-0.051905	2.998585
260.179343	2947.109294	17.418842	-0.051894	2.994820
260.123676	2939.098785	17.423847	-0.051879	2.991048
260.245138	2931.094980	17.428851	-0.051897	2.987284
260.080644	2923.121462	17.433856	-0.051862	2.983515
260.067558	2915.153326	17.438861	-0.051855	2.979751
259.885350	2907.196028	17.443866	-0.051816	2.975979
259.841953	2899.205188	17.448871	-0.051803	2.972193
259.730924	2891.225821	17.453875	-0.051778	2.968404
259.629972	2883.226708	17.458880	-0.051754	2.964602
259.650150	2875.283402	17.463885	-0.051753	2.960828
259.514847	2867.285549	17.468890	-0.051723	2.957014
259.492385	2859.286652	17.473895	-0.051715	2.953202
259.354047	2851.302685	17.478899	-0.051684	2.949385
259.267356	2843.308555	17.483904	-0.051663	2.945561
259.551574	2835.324038	17.488909	-0.051711	2.941756
259.473142	2827.335417	17.493914	-0.051692	2.937925
259.427634	2819.371261	17.498919	-0.051679	2.934103
259.250988	2811.381685	17.503923	-0.051641	2.930257
259.282074	2803.390541	17.508928	-0.051642	2.926415
259.398373	2795.432360	17.513933	-0.051659	2.922589
259.286671	2787.458241	17.518938	-0.051634	2.918739
259.351305	2779.492921	17.523943	-0.051641	2.914896
259.327490	2771.408984	17.528947	-0.051632	2.910987
258.972610	2763.451421	17.533952	-0.051561	2.907116
258.772433	2755.500557	17.538957	-0.051519	2.903251
258.783253	2747.521143	17.543962	-0.051516	2.899379
258.778251	2739.556050	17.548967	-0.051511	2.895507
258.622307	2731.587480	17.553971	-0.051477	2.891621
258.518069	2723.584308	17.558976	-0.051453	2.887715
258.621125	2715.599776	17.563981	-0.051467	2.883824
258.454421	2707.651385	17.568986	-0.051432	2.879931
258.456553	2699.676601	17.573991	-0.051427	2.876028
258.524579	2691.648010	17.578995	-0.051435	2.872098
258.305628	2683.671873	17.584000	-0.051390	2.868173
258.442052	2675.682358	17.589005	-0.051410	2.864254
258.340863	2667.728358	17.594010	-0.051387	2.860335
258.210194	2659.776583	17.599015	-0.051358	2.856410
258.133943	2651.786073	17.604019	-0.051339	2.852464
258.347474	2643.750106	17.609024	-0.051374	2.848506
258.212693	2635.812950	17.614029	-0.051344	2.844571
257.900420	2627.875374	17.619034	-0.051281	2.840621
257.929170	2619.892884	17.624039	-0.051282	2.836663
258.006316	2611.893439	17.629043	-0.051292	2.832693
257.916441	2603.880826	17.634048	-0.051270	2.828701
257.843987	2595.905771	17.639053	-0.051252	2.824724
257.639838	2587.959464	17.644058	-0.051209	2.820747
257.619863	2579.998496	17.649063	-0.051201	2.816769
257.433805	2572.010998	17.654067	-0.051161	2.812762
257.526913	2563.971942	17.659072	-0.051174	2.808739
257.538081	2556.005334	17.664077	-0.051171	2.804742
257.392412	2548.064958	17.669082	-0.051140	2.800744
257.355593	2540.103656	17.674087	-0.051128	2.796736
257.471469	2532.094117	17.679091	-0.051145	2.792706
257.151758	2524.133304	17.684096	-0.051081	2.788670
257.276374	2516.126711	17.689101	-0.051099	2.784631
257.223496	2508.179931	17.694106	-0.051085	2.780605
257.178023	2500.198281	17.699111	-0.051071	2.776557
256.940555	2492.243204	17.704115	-0.051022	2.772505
256.865805	2484.235559	17.709120	-0.051004	2.768430
257.098219	2476.246255	17.714125	-0.051042	2.764376
256.961047	2468.303693	17.719130	-0.051012	2.760319
256.676623	2460.380924	17.724135	-0.050954	2.756256
256.696734	2452.306852	17.729139	-0.050953	2.752129
256.421772	2444.315407	17.734144	-0.050897	2.748019
256.462297	2436.344639	17.739149	-0.050900	2.743934
256.546565	2428.361139	17.744154	-0.050911	2.739838
256.457469	2420.417834	17.749159	-0.050890	2.735746
256.500975	2412.426005	17.754163	-0.050893	2.731631
256.450349	2404.442202	17.759168	-0.050879	2.727509
256.649991	2396.474671	17.764173	-0.050912	2.723404
256.357837	2388.522507	17.769178	-0.050853	2.719270
256.140767	2380.592938	17.774183	-0.050807	2.715147
256.267270	2372.570961	17.779187	-0.050826	2.710990
256.107167	2364.592966	17.784192	-0.050792	2.706832
256.050750	2356.639504	17.789197	-0.050777	2.702687
256.159489	2348.648020	17.794202	-0.050792	2.698526
255.966449	2340.709116	17.799207	-0.050751	2.694367
255.746871	2332.724938	17.804211	-0.050706	2.690177
255.791235	2324.727566	17.809216	-0.050709	2.685989
256.001261	2316.764906	17.814221	-0.050744	2.681824
255.850532	2308.788534	17.819226	-0.050711	2.677622
255.745755	2300.841736	17.824231	-0.050687	2.673432
255.841062	2292.818179	17.829235	-0.050700	2.669207
255.630599	2284.849614	17.834240	-0.050656	2.664986
255.527872	2276.916109	17.839245	-0.050632	2.660783
255.457560	2268.942973	17.844250	-0.050614	2.656554
255.527627	2260.937265	17.849255	-0.050623	2.652311
255.460778	2252.977741	17.854259	-0.050605	2.648077
255.146820	2245.020132	17.859264	-0.050542	2.643820
255.298244	2237.048739	17.864269	-0.050566	2.639580
255.287114	2229.083102	17.869274	-0.050559	2.635325
255.153253	2221.092610	17.874279	-0.050529	2.631042
255.254153	2213.110230	17.879283	-0.050543	2.626772
255.026153	2205.159732	17.884288	-0.050496	2.622490
254.997816	2197.200061	17.889293	-0.050486	2.618210
254.914804	2189.225116	17.894298	-0.050466	2.613911
254.701617	2181.256295	17.899303	-0.050422	2.609599
254.774072	2173.287046	17.904307	-0.050430	2.605299
254.543031	2165.344626	17.909312	-0.050383	2.600986
254.738979	2157.362180	17.914317	-0.050415	2.596673
254.512706	2149.269880	17.919322	-0.050368	2.592264
254.476612	2141.243490	17.924327	-0.050356	2.587897
254.607926	2133.291653	17.929331	-0.050376	2.583574
254.541822	2125.366287	17.934336	-0.050359	2.579245
254.424591	2117.437262	17.939341	-0.050332	2.574903
254.277269	2109.467906	17.944346	-0.050300	2.570530
254.327877	2101.498143	17.949351	-0.050305	2.566163
254.062038	2093.572346	17.954355	-0.050251	2.561790
254.113050	2085.591695	17.959360	-0.050256	2.557402
254.195038	2077.623626	17.964365	-0.050266	2.553015
253.957705	2069.644871	17.969370	-0.050217	2.548593
253.861293	2061.688487	17.974375	-0.050195	2.544185
253.906470	2053.743196	17.979379	-0.050198	2.539785
253.988617	2045.752157	17.984384	-0.050209	2.535355
253.991336	2037.789053	17.989389	-0.050205	2.530927
253.931315	2029.817347	17.994394	-0.050189	2.526482
253.762977	2021.879383	17.999399	-0.050153	2.522041
253.788308	2013.930761	18.004403	-0.050153	2.517599
253.775135	2005.935066	18.009408	-0.050146	2.513121
253.791677	1997.945091	18.014413	-0.050144	2.508640
253.628071	1989.972232	18.019418	-0.050109	2.504147
253.571157	1982.033581	18.024423	-0.050093	2.499674
253.368793	1974.108810	18.029427	-0.050051	2.495189
253.384977	1966.101234	18.034432	-0.050049	2.490666
253.260855	1958.165144	18.039437	-0.050022	2.486164
253.176941	1950.200898	18.044442	-0.050001	2.481641
253.332076	1942.232343	18.049447	-0.050025	2.477126
253.101057	1934.275952	18.054451	-0.049978	2.472580
252.913382	1926.308735	18.059456	-0.049938	2.468023
253.178281	1918.319595	18.064461	-0.049983	2.463479
252.989384	1910.372249	18.069466	-0.049943	2.458916
252.978929	1902.423286	18.074471	-0.049936	2.454357
252.729181	1894.466058	18.079475	-0.049885	2.449767
252.842964	1886.470640	18.084480	-0.049901	2.445174
252.861249	1878.544056	18.089485	-0.049900	2.440605
252.648473	1870.599990	18.094490	-0.049856	2.435999
252.696155	1862.553057	18.099495	-0.049860	2.431345
252.605134	1854.590837	18.104499	-0.049838	2.426720
252.401042	1846.650695	18.109504	-0.049796	2.422091
252.423903	1838.711701	18.114509	-0.049795	2.417471
252.240038	1830.748880	18.119514	-0.049756	2.412813
252.152069	1822.790453	18.124519	-0.049735	2.408155
252.134628	1814.831460	18.129523	-0.049727	2.403493
252.212521	1806.850531	18.134528	-0.049737	2.398817
252.306654	1798.907882	18.139533	-0.049750	2.394156
251.928728	1790.962735	18.144538	-0.049675	2.389447
251.981902	1782.985774	18.149543	-0.049680	2.384743
252.120963	1775.035977	18.154547	-0.049701	2.380054
251.953290	1767.087763	18.159552	-0.049665	2.375331
251.672502	1759.159046	18.164557	-0.049608	2.370602
251.518035	1751.202640	18.169562	-0.049575	2.365857
251.696238	1743.230159	18.174567	-0.049603	2.361119
251.840403	1735.274213	18.179571	-0.049625	2.356379
251.529617	1727.308427	18.184576	-0.049563	2.351587
251.522661	1719.340446	18.189581	-0.049557	2.346809
251.186340	1711.402044	18.194586	-0.049489	2.342011
251.221055	1703.451933	18.199591	-0.049491	2.337227
251.341459	1695.481127	18.204595	-0.049509	2.332428
251.175272	1687.512392	18.209600	-0.049473	2.327596
251.085987	1679.593090	18.214605	-0.049452	2.322791
251.258144	1671.618949	18.219610	-0.049479	2.317963
251.227049	1663.661305	18.224615	-0.049469	2.313120
251.049552	1655.705277	18.229619	-0.049431	2.308254
250.922911	1647.762753	18.234624	-0.049403	2.303391
251.070464	1639.812287	18.239629	-0.049426	2.298536
250.790122	1631.875898	18.244634	-0.049369	2.293643
250.751380	1623.910025	18.249639	-0.049357	2.288741
250.830390	1615.954154	18.254643	-0.049367	2.283846
250.598514	1608.025486	18.259648	-0.049319	2.278930
250.610397	1600.071909	18.264653	-0.049316	2.274009
250.535648	1592.034097	18.269658	-0.049298	2.269018
250.609180	1584.078805	18.274663	-0.049307	2.264079
250.501632	1576.160610	18.279667	-0.049282	2.259138
250.365063	1568.225109	18.284672	-0.049252	2.254172
250.435653	1560.264716	18.289677	-0.049260	2.249197
250.288032	1552.328574	18.294682	-0.049228	2.244208
250.365226	1544.390044	18.299687	-0.049238	2.239226
250.160220	1536.479231	18.304691	-0.049195	2.234225
249.899325	1528.510575	18.309696	-0.049142	2.229172
250.117486	1520.543969	18.314701	-0.049178	2.224150
250.078708	1512.603359	18.319706	-0.049166	2.219111
249.972578	1504.676496	18.324711	-0.049141	2.214064
249.744644	1496.729550	18.329715	-0.049094	2.208981
249.806622	1488.759565	18.334720	-0.049101	2.203897
249.868164	1480.854500	18.339725	-0.049108	2.198844
249.591574	1472.916515	18.344730	-0.049052	2.193727
249.428741	1464.947473	18.349735	-0.049017	2.188588
249.627071	1456.973064	18.354739	-0.049049	2.183467
249.515620	1449.047040	18.359744	-0.049023	2.178337
249.373187	1441.133064	18.364749	-0.048992	2.173199
249.199142	1433.178718	18.369754	-0.048955	2.168020
249.229612	1425.236234	18.374759	-0.048956	2.162855
249.163768	1417.311562	18.379763	-0.048939	2.157681
249.110904	1409.360915	18.384768	-0.048925	2.152478
249.062879	1401.404791	18.389773	-0.048911	2.147260
248.861376	1393.481167	18.394778	-0.048869	2.142036
248.862713	1385.553904	18.399783	-0.048864	2.136815
248.862125	1377.607774	18.404787	-0.048859	2.131570
248.624783	1369.668970	18.409792	-0.048811	2.126293
248.676948	1361.740874	18.414797	-0.048816	2.121038
248.580885	1353.804459	18.419802	-0.048793	2.115751
248.601805	1345.806085	18.424807	-0.048792	2.110420
248.535237	1337.856127	18.429811	-0.048775	2.105099
248.360212	1329.957310	18.434816	-0.048738	2.099789
248.499487	1322.013877	18.439821	-0.048759	2.094466
248.160253	1314.091979	18.444826	-0.048691	2.089097
248.074211	1306.174518	18.449831	-0.048671	2.083742
248.058999	1298.252202	18.454835	-0.048663	2.078377
247.901621	1290.311515	18.459840	-0.048629	2.072971
247.871396	1282.374961	18.464845	-0.048619	2.067567
247.725984	1274.443505	18.469850	-0.048587	2.062140
247.629757	1266.546570	18.474855	-0.048564	2.056728
247.708231	1258.586763	18.479859	-0.048574	2.051276
247.709102	1250.628113	18.484864	-0.048570	2.045802
247.809179	1242.716208	18.489869	-0.048584	2.040356
247.271060	1234.865535	18.494874	-0.048479	2.034873
247.329309	1226.875734	18.499879	-0.048485	2.029339
247.268127	1218.951231	18.504883	-0.048469	2.023823
247.169445	1211.022127	18.509888	-0.048446	2.018285
247.307205	1203.077509	18.514893	-0.048467	2.012745
247.098895	1195.159932	18.519898	-0.048423	2.007174
246.999728	1187.257206	18.524903	-0.048400	2.001608
246.960110	1179.354426	18.529907	-0.048388	1.996033
246.979799	1171.385995	18.534912	-0.048387	1.990402
247.132480	1163.437473	18.539917	-0.048411	1.984783
246.934045	1155.550347	18.544922	-0.048369	1.979155
246.875318	1147.642908	18.549927	-0.048354	1.973512
246.695407	1139.725593	18.554931	-0.048315	1.967832
246.632527	1131.807049	18.559936	-0.048299	1.962147
246.551163	1123.930275	18.564941	-0.048279	1.956473
246.410500	1115.959484	18.569946	-0.048248	1.950709
246.429829	1108.011421	18.574951	-0.048247	1.944962
246.451514	1100.101487	18.579955	-0.048247	1.939225
246.278797	1092.194415	18.584960	-0.048210	1.933453
246.129980	1084.292954	18.589965	-0.048177	1.927669
246.300746	1076.341836	18.594970	-0.048205	1.921867
246.127387	1068.468560	18.599975	-0.048168	1.916067
246.098451	1060.537970	18.604979	-0.048158	1.910223
246.078704	1052.608942	18.609984	-0.048149	1.904363
245.919764	1044.740301	18.614989	-0.048115	1.898514
245.755623	1036.830754	18.619994	-0.048080	1.892616
245.749759	1028.910035	18.624999	-0.048074	1.886709
245.618654	1021.022701	18.630003	-0.048045	1.880794
245.448085	1013.123267	18.635008	-0.048008	1.874847
245.588035	1005.174172	18.640013	-0.048030	1.868879
245.462206	997.261746	18.645018	-0.048002	1.862889
245.410813	989.377254	18.650023	-0.047987	1.856910
245.371024	981.470871	18.655027	-0.047975	1.850896
245.391387	973.541938	18.660032	-0.047974	1.844852
245.466523	965.652531	18.665037	-0.047984	1.838825
245.309773	957.764580	18.670042	-0.047950	1.832752
245.215222	949.852845	18.675047	-0.047928	1.826647
245.213504	941.959969	18.680051	-0.047923	1.820548
245.018850	934.093076	18.685056	-0.047882	1.814426
244.733994	926.218909	18.690061	-0.047824	1.808266
244.615975	918.335639	18.695066	-0.047797	1.802098
244.770464	910.416792	18.700071	-0.047822	1.795914
244.766707	902.455169	18.705075	-0.047816	1.789655
244.675035	894.559475	18.710080	-0.047794	1.783416
244.591860	886.698396	18.715085	-0.047774	1.777184
244.256715	878.835815	18.720090	-0.047707	1.770897
244.368097	870.920212	18.725095	-0.047723	1.764601
244.392758	863.043100	18.730099	-0.047723	1.758302
244.124477	855.178703	18.735104	-0.047669	1.751954
244.206018	847.263436	18.740109	-0.047679	1.745587
244.101188	839.399128	18.745114	-0.047655	1.739213
244.051952	831.519867	18.750119	-0.047641	1.732811
244.149714	823.603077	18.755123	-0.047655	1.726373
243.964515	815.759313	18.760128	-0.047616	1.719935
243.960519	807.896263	18.765133	-0.047610	1.713480
243.549930	800.039027	18.770138	-0.047529	1.706952
243.511157	792.156638	18.775143	-0.047517	1.700427
243.585051	784.270579	18.780147	-0.047526	1.693889
243.257929	776.421155	18.785152	-0.047461	1.687303
243.203727	768.553354	18.790157	-0.047446	1.680712
243.145076	760.684106	18.795162	-0.047431	1.674093
243.199344	752.776369	18.800167	-0.047436	1.667430
243.323829	744.896887	18.805171	-0.047454	1.660774
243.051171	737.070670	18.810176	-0.047399	1.654083
243.058534	729.203148	18.815181	-0.047396	1.647367
242.797634	721.363287	18.820186	-0.047343	1.640611
242.785282	713.499647	18.825191	-0.047336	1.633841
242.889987	705.568043	18.830195	-0.047350	1.627000
242.708398	697.733318	18.835200	-0.047312	1.620174
242.605519	689.902874	18.840205	-0.047288	1.613334
242.627022	682.015108	18.845210	-0.047288	1.606432
242.347062	674.216582	18.850215	-0.047231	1.599537
242.396918	666.356788	18.855219	-0.047236	1.592604
242.414946	658.473683	18.860224	-0.047234	1.585616
242.395787	650.653600	18.865229	-0.047226	1.578647
242.296479	642.806228	18.870234	-0.047203	1.571612
242.071814	634.995534	18.875239	-0.047157	1.564559
241.971530	627.187366	18.880243	-0.047133	1.557496
242.002663	619.302729	18.885248	-0.047134	1.550349
241.943802	611.471119	18.890253	-0.047119	1.543205
241.633358	603.684555	18.895258	-0.047056	1.536031
241.678897	595.823008	18.900263	-0.047060	1.528808
241.655922	587.992921	18.905267	-0.047051	1.521570
241.478884	580.190209	18.910272	-0.047014	1.514298
241.623816	572.322405	18.915277	-0.047036	1.506980
241.426625	564.529075	18.920282	-0.046995	1.499644
241.311468	556.733517	18.925287	-0.046969	1.492282
241.266711	548.906740	18.930291	-0.046956	1.484865
240.997246	541.141394	18.935296	-0.046901	1.477434
241.123673	533.260936	18.940301	-0.046920	1.469918
240.977368	525.450035	18.945306	-0.046888	1.462386
240.773187	517.677669	18.950311	-0.046845	1.454844
240.743823	509.861870	18.955315	-0.046835	1.447248
240.520339	502.088048	18.960320	-0.046789	1.439622
240.574979	494.283428	18.965325	-0.046795	1.431969
240.313883	486.507123	18.970330	-0.046742	1.424253
240.214030	478.733054	18.975335	-0.046718	1.416522
240.130058	470.942634	18.980339	-0.046698	1.408736
240.244507	463.131083	18.985344	-0.046715	1.400918
240.125140	455.378315	18.990349	-0.046688	1.393076
240.215908	447.551367	18.995354	-0.046700	1.385151
240.015342	439.816290	19.000359	-0.046658	1.377223
239.885399	432.046351	19.005363	-0.046630	1.369227
239.804242	424.282513	19.010368	-0.046610	1.361197
239.921588	416.511736	19.015373	-0.046627	1.353148
239.512797	408.784417	19.020378	-0.046547	1.345004
239.437556	401.044380	19.025383	-0.046528	1.336855
239.372726	393.294053	19.030387	-0.046511	1.328647
239.405565	385.535498	19.035392	-0.046513	1.320397
239.272136	377.765913	19.040397	-0.046484	1.312053
239.107699	369.963348	19.045402	-0.046448	1.303615
239.158573	362.231930	19.050407	-0.046453	1.295238
238.970885	354.530413	19.055411	-0.046414	1.286795
238.856924	346.827206	19.060416	-0.046388	1.278309
238.964640	339.098123	19.065421	-0.046403	1.269778
238.653503	331.419876	19.070426	-0.046341	1.261168
238.459577	323.749097	19.075431	-0.046300	1.252529
238.452266	316.031945	19.080435	-0.046294	1.243813
238.408386	308.336456	19.085440	-0.046282	1.235053
238.401755	300.627193	19.090445	-0.046276	1.226222
238.107092	292.987563	19.095450	-0.046217	1.217351
238.071302	285.300954	19.100455	-0.046205	1.208411
237.873714	277.658534	19.105459	-0.046164	1.199425
237.734951	269.998222	19.110464	-0.046134	1.190360
237.573174	262.356225	19.115469	-0.046099	1.181244
237.571089	254.688251	19.120474	-0.046094	1.172058
237.340635	247.072026	19.125479	-0.046047	1.162815
237.192626	239.448565	19.130483	-0.046015	1.153506
237.019395	231.785672	19.135488	-0.045978	1.144067
237.061520	224.158508	19.140493	-0.045981	1.134640
236.774524	216.566429	19.145498	-0.045924	1.125107
236.567741	208.991185	19.150503	-0.045881	1.115531
236.487836	201.378433	19.155507	-0.045861	1.105853
236.062135	193.849449	19.160512	-0.045778	1.096120
235.984487	186.258274	19.165517	-0.045759	1.086296
235.545554	178.751954	19.170522	-0.045672	1.076413
235.248687	171.195682	19.175527	-0.045613	1.066404
234.800018	163.701799	19.180531	-0.045525	1.056348
234.511326	156.160152	19.185536	-0.045467	1.046168
234.148803	148.679393	19.190541	-0.045395	1.035954
233.676316	141.186573	19.195546	-0.045302	1.025595
233.206082	133.731388	19.200551	-0.045210	1.015182
232.730171	126.273452	19.205555	-0.045117	1.004657
232.322963	118.812768	19.210560	-0.045037	0.994032
232.056115	111.317387	19.215565	-0.044983	0.983278
231.724739	103.867637	19.220570	-0.044917	0.972455
231.139717	96.483244	19.225575	-0.044804	0.961541
231.018286	89.035960	19.230579	-0.044777	0.950528
230.672678	81.632619	19.235584	-0.044708	0.939392
230.167109	74.287654	19.240589	-0.044610	0.928169
229.599372	66.964840	19.245594	-0.044500	0.916826
228.956722	59.885149	19.250599	-0.044376	0.905699