Tue Mar 23 10:23:43 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.857563	-0.008093	0.000000	-0.000028	0.725263

0.632028	0.009577	0.005005	0.000013	0.725219
0.650922	0.008761	0.010010	0.000010	0.725225
0.762032	-0.011779	0.015014	-0.000011	0.725223
0.823518	-0.025482	0.020019	-0.000023	0.725218
0.730679	-0.006331	0.025024	-0.000006	0.725224
0.740162	-0.010858	0.030029	-0.000008	0.725219
0.676423	0.005308	0.035034	0.000004	0.725229
0.687205	-0.001685	0.040038	0.000002	0.725219
0.801354	-0.021449	0.045043	-0.000020	0.725221
0.559918	0.024908	0.050048	0.000025	0.725228
0.559126	0.019098	0.055053	0.000025	0.725216
0.667894	0.003283	0.060058	0.000004	0.725224
0.727039	-0.009764	0.065062	-0.000007	0.725219
0.756971	-0.015616	0.070067	-0.000013	0.725219
0.787602	-0.061214	0.075072	-0.000019	0.725141
0.768586	-0.186762	0.080077	-0.000015	0.724889
0.635805	-0.159425	0.085082	0.000009	0.724896
0.551169	-0.144886	0.090086	0.000025	0.724896
0.661791	-0.165499	0.095091	0.000004	0.724894
0.809776	-0.188376	0.100096	-0.000024	0.724901
0.681809	-0.169354	0.105101	-0.000000	0.724895
0.728448	-0.288124	0.110106	-0.000009	0.724679
0.632672	-0.312269	0.115110	0.000009	0.724598
0.654891	-0.315752	0.120115	0.000004	0.724600
0.766280	-0.330960	0.125120	-0.000017	0.724609
0.484813	-0.285611	0.130125	0.000036	0.724600
0.435761	-0.389974	0.135130	0.000045	0.724379
0.479086	-0.452808	0.140134	0.000036	0.724272
0.486114	-0.456656	0.145139	0.000035	0.724267
0.657472	-0.482541	0.150144	0.000003	0.724277
0.503789	-0.502212	0.155149	0.000031	0.724185
0.597487	-0.632119	0.160154	0.000013	0.723963
0.488296	-0.611933	0.165158	0.000034	0.723965
0.334513	-0.586278	0.170163	0.000062	0.723962
0.605310	-0.702675	0.175168	0.000011	0.723829
0.603160	-0.799459	0.180173	0.000012	0.723639
0.531315	-0.785005	0.185178	0.000025	0.723643
0.443988	-0.771418	0.190182	0.000041	0.723639
0.383698	-0.909928	0.195187	0.000052	0.723347
0.601957	-0.945762	0.200192	0.000011	0.723353
0.359952	-0.906152	0.205197	0.000056	0.723347
0.610244	-1.089784	0.210202	0.000009	0.723075
0.678003	-1.132923	0.215206	-0.000004	0.723014
0.459393	-1.094332	0.220211	0.000037	0.723014
0.394650	-1.232874	0.225216	0.000049	0.722720
0.510082	-1.263610	0.230221	0.000027	0.722700
0.560549	-1.301865	0.235226	0.000018	0.722643
0.644777	-1.450714	0.240230	0.000002	0.722381
0.463782	-1.420885	0.245235	0.000035	0.722376
0.490719	-1.515858	0.250240	0.000030	0.722200
0.414824	-1.563264	0.255245	0.000044	0.722080
0.286854	-1.561267	0.260250	0.000068	0.722040
0.142832	-1.681322	0.265254	0.000094	0.721754
0.146548	-1.684056	0.270259	0.000093	0.721750
0.073961	-1.771594	0.275264	0.000107	0.721553
0.047449	-1.820551	0.280269	0.000112	0.721448
0.222382	-1.897586	0.285274	0.000079	0.721358
0.104155	-1.990037	0.290278	0.000101	0.721135
0.193143	-2.015172	0.295283	0.000084	0.721118
0.136920	-2.121520	0.300288	0.000094	0.720889
-0.002838	-2.100334	0.305293	0.000120	0.720882
-0.072067	-2.229663	0.310298	0.000133	0.720604
-0.178609	-2.239128	0.315302	0.000152	0.720548
-0.166924	-2.352638	0.320307	0.000150	0.720329
-0.300689	-2.375275	0.325312	0.000175	0.720238
-0.639726	-2.411713	0.330317	0.000238	0.720048
-3.685573	-1.940424	0.335322	0.000804	0.719908
-2.855733	-2.089613	0.340326	0.000650	0.719906
-3.363814	-2.073686	0.345331	0.000744	0.719759
-4.556195	-1.937283	0.350336	0.000966	0.719610
-4.005368	-2.039645	0.355341	0.000863	0.719602
-3.789550	-2.074993	0.360346	0.000823	0.719609
-4.768735	-2.047334	0.365350	0.001005	0.719320
-5.243901	-1.989484	0.370355	0.001093	0.719267
-5.118439	-2.006648	0.375360	0.001069	0.719278
-5.297226	-1.980638	0.380365	0.001102	0.719267
-5.249753	-2.076772	0.385370	0.001094	0.719094
-5.984995	-2.011760	0.390374	0.001230	0.718965
-6.135289	-1.986430	0.395379	0.001258	0.718962
-6.060594	-1.993964	0.400384	0.001244	0.718974
-5.970837	-2.016085	0.405389	0.001227	0.718962
-6.374176	-2.099793	0.410394	0.001302	0.718656
-6.948573	-2.000089	0.415398	0.001408	0.718651
-7.120756	-1.970029	0.420403	0.001440	0.718650
-6.445089	-2.086914	0.425408	0.001314	0.718657
-7.062071	-1.985438	0.430413	0.001429	0.718641
-7.836064	-1.987616	0.435418	0.001573	0.718365
-7.720165	-2.007829	0.440422	0.001551	0.718366
-7.739447	-2.005944	0.445427	0.001554	0.718364
-7.601273	-2.027041	0.450432	0.001529	0.718371
-7.728696	-2.009891	0.455437	0.001552	0.718361
-7.702595	-2.113364	0.460442	0.001547	0.718166
-9.037996	-1.945961	0.465446	0.001795	0.718027
-8.899342	-1.973189	0.470451	0.001769	0.718023
-8.437859	-2.053481	0.475456	0.001683	0.718027
-8.733669	-2.003696	0.480461	0.001738	0.718021
-8.652230	-2.015402	0.485466	0.001723	0.718027
-8.803903	-2.088197	0.490470	0.001751	0.717830
-9.853482	-1.962454	0.495475	0.001946	0.717710
-9.637434	-1.996436	0.500480	0.001905	0.717719
-9.684989	-1.993109	0.505485	0.001914	0.717709
-9.557231	-2.012394	0.510490	0.001890	0.717717
-9.513447	-2.021187	0.515494	0.001882	0.717715
-9.846125	-2.023613	0.520499	0.001944	0.717594
-10.470239	-2.013906	0.525504	0.002059	0.717393
-10.427527	-2.025033	0.530509	0.002051	0.717387
-10.685336	-1.978064	0.535514	0.002099	0.717389
-10.639341	-1.986737	0.540518	0.002090	0.717389
-10.548898	-2.005536	0.545523	0.002073	0.717384
-10.518076	-2.007600	0.550528	0.002067	0.717391
-11.070648	-2.016204	0.555533	0.002170	0.717180
-11.428774	-1.997205	0.560538	0.002236	0.717092
-11.350309	-2.010754	0.565542	0.002222	0.717093
-12.047583	-1.889465	0.570547	0.002351	0.717088
-11.592856	-1.964263	0.575552	0.002266	0.717100
-11.257433	-2.030673	0.580557	0.002204	0.717087
-11.545584	-1.975776	0.585562	0.002257	0.717095
-11.705688	-2.045353	0.590566	0.002287	0.716901
-12.810276	-1.919930	0.595571	0.002492	0.716760
-12.365987	-1.996304	0.600576	0.002409	0.716766
-12.463897	-1.982345	0.605581	0.002427	0.716760
-12.200615	-2.025852	0.610586	0.002378	0.716767
-12.312003	-2.006536	0.615590	0.002399	0.716766
-12.535577	-1.969921	0.620595	0.002440	0.716760
-12.479953	-2.066952	0.625600	0.002429	0.716588
-13.576103	-1.943192	0.630605	0.002633	0.716447
-13.408964	-1.969579	0.635610	0.002602	0.716454
-13.421809	-1.967458	0.640614	0.002604	0.716454
-13.434639	-1.966876	0.645619	0.002606	0.716451
-13.238546	-1.998380	0.650624	0.002570	0.716459
-13.439133	-1.966842	0.655629	0.002607	0.716451
-13.381143	-2.026630	0.660634	0.002596	0.716353
-14.154402	-1.996351	0.665638	0.002739	0.716141
-14.381940	-1.959262	0.670643	0.002782	0.716134
-14.324011	-1.966398	0.675648	0.002771	0.716141
-14.183282	-1.995843	0.680653	0.002744	0.716133
-14.221933	-1.987117	0.685658	0.002751	0.716137
-14.353416	-1.964772	0.690662	0.002775	0.716135
-14.473063	-1.950916	0.695667	0.002797	0.716121
-14.642759	-2.036441	0.700672	0.002829	0.715892
-15.125284	-1.953149	0.705677	0.002918	0.715887
-15.073055	-1.961357	0.710682	0.002909	0.715889
-14.717164	-2.025185	0.715686	0.002842	0.715889
-15.261793	-1.931107	0.720691	0.002943	0.715884
-15.085836	-1.958085	0.725696	0.002910	0.715893
-15.114020	-1.998351	0.730701	0.002915	0.715803
-16.083829	-1.954657	0.735706	0.003096	0.715548
-15.928729	-1.981819	0.740710	0.003067	0.715549
-16.298162	-1.918233	0.745715	0.003135	0.715545
-16.134427	-1.941226	0.750720	0.003104	0.715558
-16.315687	-1.914067	0.755725	0.003138	0.715548
-16.216236	-1.929822	0.760730	0.003119	0.715552
-15.815055	-2.001048	0.765734	0.003044	0.715553
-16.624459	-1.991696	0.770739	0.003195	0.715286
-17.024550	-1.942277	0.775744	0.003269	0.715243
-17.006273	-1.950852	0.780749	0.003265	0.715233
-16.897445	-1.967059	0.785754	0.003245	0.715240
-17.200168	-1.913543	0.790758	0.003301	0.715239
-17.213672	-1.913113	0.795763	0.003303	0.715236
-16.850009	-1.974316	0.800768	0.003236	0.715243
-17.421586	-1.933643	0.805773	0.003342	0.715122
-18.027723	-1.931155	0.810778	0.003454	0.714914
-17.455832	-2.031769	0.815782	0.003348	0.714916
-18.164838	-1.909150	0.820787	0.003479	0.714910
-18.026196	-1.929096	0.825792	0.003453	0.714919
-17.908689	-1.956601	0.830797	0.003431	0.714907
-18.019588	-1.933909	0.835802	0.003452	0.714913
-17.939189	-1.948750	0.840806	0.003437	0.714912
-18.544019	-1.994095	0.845811	0.003549	0.714609
-18.687660	-1.965768	0.850816	0.003576	0.714615
-19.180749	-1.880660	0.855821	0.003667	0.714610
-18.781927	-1.949389	0.860826	0.003593	0.714615
-18.448606	-2.009281	0.865830	0.003530	0.714614
-19.070407	-1.901718	0.870835	0.003646	0.714608
-18.851256	-1.937266	0.875840	0.003605	0.714615
-18.978468	-2.046089	0.880845	0.003628	0.714355
-19.874945	-1.924480	0.885850	0.003795	0.714279
-19.794803	-1.937193	0.890854	0.003780	0.714283
-19.607877	-1.973170	0.895859	0.003745	0.714278
-19.559096	-1.977902	0.900864	0.003736	0.714286
-19.773233	-1.944953	0.905869	0.003775	0.714276
-19.909524	-1.918722	0.910874	0.003800	0.714281
-19.884463	-2.011173	0.915878	0.003796	0.714106
-21.135798	-1.859397	0.920883	0.004028	0.713965
-20.414709	-1.982946	0.925888	0.003894	0.713975
-20.589427	-1.956230	0.930893	0.003926	0.713967
-20.578411	-1.955336	0.935898	0.003924	0.713973
-20.382047	-1.990363	0.940902	0.003887	0.713974
-20.747264	-1.927123	0.945907	0.003955	0.713970
-20.531222	-2.042760	0.950912	0.003915	0.713817
-21.846668	-1.890635	0.955917	0.004159	0.713654
-21.487842	-1.950835	0.960922	0.004092	0.713662
-21.316834	-1.983269	0.965926	0.004060	0.713659
-21.833452	-1.893765	0.970931	0.004156	0.713654
-21.699078	-1.913433	0.975936	0.004131	0.713663
-21.578580	-1.940323	0.980941	0.004108	0.713652
-21.502286	-1.969660	0.985946	0.004094	0.713622
-22.254503	-1.964994	0.990950	0.004234	0.713365
-22.434494	-1.934628	0.995955	0.004267	0.713362
-22.269745	-1.962141	1.000960	0.004236	0.713366
-22.424866	-1.937735	1.005965	0.004265	0.713360
-22.532107	-1.917818	1.010970	0.004284	0.713362
-22.292844	-1.959939	1.015974	0.004240	0.713363
-22.353715	-1.961345	1.020979	0.004251	0.713339
-23.251839	-1.957058	1.025984	0.004418	0.713030
-23.496280	-1.916660	1.030989	0.004463	0.713024
-23.513498	-1.911564	1.035994	0.004466	0.713028
-23.249287	-1.957699	1.040998	0.004417	0.713031
-23.676660	-1.888634	1.046003	0.004496	0.713017
-23.183625	-1.970828	1.051008	0.004404	0.713029
-23.145114	-1.981031	1.056013	0.004397	0.713022
-23.533657	-2.019043	1.061018	0.004469	0.712809
-24.243996	-1.939503	1.066022	0.004601	0.712716
-24.008164	-1.986738	1.071027	0.004557	0.712706
-23.974093	-1.987762	1.076032	0.004550	0.712717
-24.510499	-1.895781	1.081037	0.004650	0.712710
-24.181737	-1.952555	1.086042	0.004588	0.712714
-24.247566	-1.938918	1.091046	0.004600	0.712718
-24.670051	-1.975417	1.096051	0.004679	0.712496
-25.090619	-1.951314	1.101056	0.004757	0.712395
-25.137082	-1.947552	1.106061	0.004765	0.712386
-25.604690	-1.862339	1.111066	0.004852	0.712391
-25.263906	-1.922315	1.116070	0.004789	0.712393
-25.217079	-1.934623	1.121075	0.004780	0.712385
-25.196342	-1.934372	1.126080	0.004776	0.712393
-25.569043	-1.868691	1.131085	0.004845	0.712392
-25.538708	-2.022612	1.136090	0.004839	0.712097
-25.646156	-2.005203	1.141094	0.004859	0.712094
-26.432204	-1.869758	1.146099	0.005005	0.712085
-25.862419	-1.964660	1.151104	0.004899	0.712099
-25.912048	-1.959392	1.156109	0.004908	0.712092
-26.138574	-1.918537	1.161114	0.004950	0.712093
-25.773694	-2.017653	1.166118	0.004881	0.712026
-26.862302	-1.955675	1.171123	0.005084	0.711763
-26.940816	-1.937745	1.176128	0.005098	0.711771
-27.234043	-1.890485	1.181133	0.005153	0.711762
-27.039725	-1.924841	1.186138	0.005116	0.711763
-26.836531	-1.958547	1.191142	0.005078	0.711768
-27.483342	-1.846298	1.196147	0.005198	0.711762
-27.064762	-1.916498	1.201152	0.005120	0.711772
-26.965543	-2.032363	1.206157	0.005102	0.711576
-28.202210	-1.870340	1.211162	0.005332	0.711460
-27.875710	-1.926603	1.216166	0.005271	0.711464
-27.636450	-1.971900	1.221171	0.005226	0.711460
-27.838105	-1.933676	1.226176	0.005263	0.711465
-28.037247	-1.899576	1.231181	0.005300	0.711462
-27.832661	-1.935019	1.236186	0.005262	0.711465
-28.045208	-1.971830	1.241190	0.005301	0.711316
-29.340243	-1.826322	1.246195	0.005542	0.711146
-28.785009	-1.922714	1.251200	0.005438	0.711152
-28.569310	-1.967997	1.256205	0.005398	0.711138
-28.972852	-1.892670	1.261210	0.005473	0.711146
-28.648682	-1.950514	1.266214	0.005412	0.711146
-28.743887	-1.935361	1.271219	0.005430	0.711143
-28.720317	-1.968699	1.276224	0.005425	0.711085
-29.608037	-1.916717	1.281229	0.005590	0.710873
-29.460003	-1.942165	1.286234	0.005563	0.710876
-29.535457	-1.928458	1.291238	0.005576	0.710877
-29.750320	-1.893548	1.296243	0.005616	0.710870
-29.583255	-1.920315	1.301248	0.005585	0.710877
-29.482521	-1.938781	1.306253	0.005566	0.710876
-29.431484	-2.021122	1.311258	0.005556	0.710730
-30.691536	-1.892820	1.316262	0.005791	0.710538
-30.313547	-1.963967	1.321267	0.005720	0.710531
-30.306067	-1.960388	1.326272	0.005718	0.710541
-30.662366	-1.901175	1.331277	0.005785	0.710533
-30.560081	-1.918941	1.336282	0.005765	0.710535
-30.297605	-1.962592	1.341286	0.005716	0.710541
-30.961365	-1.910665	1.346291	0.005840	0.710409
-31.434266	-1.917955	1.351296	0.005927	0.710227
-31.067970	-1.988267	1.356301	0.005859	0.710217
-31.520025	-1.906445	1.361306	0.005943	0.710220
-31.427702	-1.921304	1.366310	0.005926	0.710224
-31.240028	-1.959752	1.371315	0.005890	0.710214
-31.228249	-1.956044	1.376320	0.005888	0.710226
-31.569245	-1.960265	1.381325	0.005951	0.710096
-32.583530	-1.880844	1.386330	0.006140	0.709894
-32.108313	-1.964670	1.391334	0.006051	0.709896
-32.570728	-1.885839	1.396339	0.006137	0.709890
-32.463131	-1.899324	1.401344	0.006117	0.709901
-32.124817	-1.963518	1.406349	0.006054	0.709894
-32.182025	-1.952204	1.411354	0.006064	0.709897
-32.474022	-1.903660	1.416358	0.006118	0.709890
-33.069208	-1.945189	1.421363	0.006229	0.709595
-32.791112	-1.989564	1.426368	0.006177	0.709606
-33.485105	-1.870169	1.431373	0.006306	0.709598
-33.312541	-1.901748	1.436378	0.006273	0.709597
-32.953354	-1.963107	1.441382	0.006206	0.709602
-33.269114	-1.911419	1.446387	0.006265	0.709594
-33.246041	-1.913123	1.451392	0.006260	0.709599
-33.721523	-1.984729	1.456397	0.006349	0.709287
-34.354657	-1.884167	1.461402	0.006466	0.709262
-34.337242	-1.883304	1.466406	0.006463	0.709271
-33.770637	-1.990009	1.471411	0.006357	0.709260
-33.873796	-1.966920	1.476416	0.006376	0.709270
-34.403149	-1.874635	1.481421	0.006475	0.709266
-34.155833	-1.918831	1.486426	0.006428	0.709266
-34.062501	-2.040890	1.491430	0.006411	0.709055
-35.303693	-1.872429	1.496435	0.006642	0.708950
-35.251141	-1.876816	1.501440	0.006632	0.708961
-35.010417	-1.922878	1.506445	0.006587	0.708955
-35.215975	-1.885832	1.511450	0.006625	0.708956
-35.019475	-1.918442	1.516454	0.006588	0.708961
-35.387869	-1.857953	1.521459	0.006656	0.708951
-35.295670	-1.899296	1.526464	0.006639	0.708902
-35.783078	-1.944226	1.531469	0.006729	0.708638
-35.616590	-1.973515	1.536474	0.006698	0.708639
-35.794187	-1.940321	1.541478	0.006731	0.708643
-36.072543	-1.893068	1.546483	0.006783	0.708639
-35.741859	-1.948188	1.551488	0.006721	0.708647
-35.920872	-1.916612	1.556493	0.006754	0.708646
-35.956120	-1.962227	1.561498	0.006760	0.708543
-36.640838	-1.932717	1.566502	0.006888	0.708358
-36.865167	-1.895790	1.571507	0.006929	0.708352
-36.840108	-1.895088	1.576512	0.006924	0.708363
-36.684831	-1.926702	1.581517	0.006895	0.708355
-36.680529	-1.927558	1.586522	0.006894	0.708356
-36.769035	-1.910357	1.591526	0.006910	0.708359
-36.633131	-1.994859	1.596531	0.006885	0.708238
-37.558654	-1.939323	1.601536	0.007057	0.708020
-37.624375	-1.928285	1.606541	0.007069	0.708019
-37.930106	-1.872608	1.611546	0.007126	0.708021
-37.914874	-1.875645	1.616550	0.007123	0.708021
-37.989113	-1.864762	1.621555	0.007136	0.708017
-37.788898	-1.897767	1.626560	0.007099	0.708023
-37.642657	-1.926524	1.631565	0.007071	0.708018
-38.456782	-1.929044	1.636570	0.007223	0.707722
-38.374680	-1.950533	1.641574	0.007207	0.707709
-38.769748	-1.884148	1.646579	0.007281	0.707701
-38.304024	-1.964665	1.651584	0.007194	0.707706
-38.670429	-1.900509	1.656589	0.007262	0.707705
-38.406587	-1.950029	1.661594	0.007212	0.707700
-38.288560	-1.979009	1.666598	0.007190	0.707684
-39.277198	-1.953737	1.671603	0.007374	0.707382
-39.299740	-1.945726	1.676608	0.007378	0.707390
-39.381660	-1.934483	1.681613	0.007393	0.707384
-39.566974	-1.901819	1.686618	0.007427	0.707384
-39.305101	-1.946128	1.691622	0.007378	0.707389
-39.515182	-1.915466	1.696627	0.007417	0.707376
-39.478078	-1.925240	1.701632	0.007410	0.707370
-40.430993	-1.895298	1.706637	0.007587	0.707089
-40.249520	-1.929205	1.711642	0.007553	0.707087
-40.006331	-1.971391	1.716646	0.007508	0.707089
-40.328943	-1.916629	1.721651	0.007568	0.707084
-40.036365	-1.966723	1.726656	0.007513	0.707089
-40.067876	-1.962907	1.731661	0.007519	0.707086
-40.340693	-1.946867	1.736666	0.007569	0.707021
-40.994163	-1.959805	1.741670	0.007691	0.706761
-41.067542	-1.950274	1.746675	0.007704	0.706754
-41.285923	-1.907870	1.751680	0.007745	0.706762
-41.374911	-1.894393	1.756685	0.007761	0.706757
-41.141428	-1.936598	1.761690	0.007717	0.706757
-40.966774	-1.965639	1.766694	0.007685	0.706761
-41.541721	-1.878334	1.771699	0.007791	0.706731
-41.950829	-1.942530	1.776704	0.007867	0.706456
-41.723320	-1.985575	1.781709	0.007825	0.706451
-42.528938	-1.842590	1.786714	0.007974	0.706451
-41.930725	-1.948595	1.791718	0.007863	0.706452
-42.051838	-1.931449	1.796723	0.007885	0.706444
-42.163601	-1.907931	1.801728	0.007906	0.706451
-42.318336	-1.881375	1.806733	0.007934	0.706450
-42.503536	-1.982353	1.811738	0.007969	0.706181
-42.982804	-1.918293	1.816742	0.008058	0.706138
-43.364843	-1.855184	1.821747	0.008129	0.706129
-42.652810	-1.977519	1.826752	0.007996	0.706138
-42.974942	-1.923224	1.831757	0.008056	0.706132
-43.324157	-1.863131	1.836762	0.008120	0.706129
-42.920861	-1.932110	1.841766	0.008045	0.706135
-43.132946	-1.985788	1.846771	0.008084	0.705951
-43.798344	-1.910079	1.851776	0.008208	0.705865
-43.657840	-1.937344	1.856781	0.008182	0.705861
-43.643871	-1.939846	1.861786	0.008179	0.705862
-43.541025	-1.954309	1.866790	0.008160	0.705870
-43.899274	-1.895591	1.871795	0.008226	0.705860
-44.099634	-1.853065	1.876800	0.008263	0.705874
-44.342717	-1.971415	1.881805	0.008308	0.705549
-44.632047	-1.930755	1.886810	0.008362	0.705528
-44.512146	-1.948880	1.891814	0.008339	0.705535
-44.517967	-1.954369	1.896819	0.008340	0.705522
-44.781474	-1.901716	1.901824	0.008389	0.705534
-44.924805	-1.878391	1.906829	0.008415	0.705530
-44.709283	-1.918291	1.911834	0.008375	0.705527
-45.022742	-2.015060	1.916838	0.008433	0.705220
-45.876599	-1.866100	1.921843	0.008592	0.705214
-45.773435	-1.882562	1.926848	0.008573	0.705218
-45.233945	-1.980205	1.931853	0.008472	0.705216
-45.551332	-1.924189	1.936858	0.008531	0.705215
-45.762639	-1.884523	1.941862	0.008570	0.705220
-45.763288	-1.888179	1.946867	0.008570	0.705212
-46.047332	-1.978729	1.951872	0.008623	0.704928
-46.670446	-1.885381	1.956877	0.008738	0.704893
-46.740281	-1.876200	1.961882	0.008751	0.704887
-46.321183	-1.945490	1.966886	0.008673	0.704898
-46.731005	-1.877839	1.971891	0.008749	0.704888
-46.494906	-1.917107	1.976896	0.008705	0.704894
-46.189631	-1.974128	1.981901	0.008648	0.704889
-46.830201	-1.974883	1.986906	0.008767	0.704658
-47.516682	-1.881576	1.991910	0.008894	0.704600
-47.386569	-1.909428	1.996915	0.008870	0.704591
-47.311581	-1.920103	2.001920	0.008856	0.704597

-47.377499	-1.906322	2.011917	0.008868	0.704602
-47.679098	-1.853751	2.021914	0.008923	0.704600
-47.682983	-1.925694	2.031910	0.008924	0.704454
-48.370672	-1.876278	2.041907	0.009051	0.704308
-48.041531	-1.887105	2.051904	0.008990	0.704405
-47.544209	-1.944262	2.061901	0.008897	0.704469
-47.498280	-1.939951	2.071898	0.008888	0.704495
-47.359495	-1.916756	2.081894	0.008861	0.704593
-47.639758	-1.866010	2.091891	0.008913	0.704595
-47.280814	-1.931022	2.101888	0.008846	0.704594
-47.399046	-1.910360	2.111885	0.008867	0.704594
-47.554696	-1.882058	2.121882	0.008896	0.704596
-47.375217	-1.914345	2.131878	0.008862	0.704596
-47.422846	-1.906810	2.141875	0.008870	0.704595
-46.668543	-1.930223	2.151872	0.008730	0.704820
-46.672182	-1.893410	2.161869	0.008730	0.704893
-46.441335	-1.935124	2.171866	0.008686	0.704893
-46.454166	-1.934645	2.181862	0.008688	0.704890
-46.790699	-1.847570	2.191859	0.008751	0.704946
-45.729125	-1.904269	2.201856	0.008552	0.705213
-45.621694	-1.921967	2.211853	0.008532	0.705217
-45.694542	-1.910442	2.221850	0.008545	0.705215
-45.498097	-1.929878	2.231846	0.008508	0.705247
-44.873697	-1.901216	2.241843	0.008391	0.705530
-44.699987	-1.931541	2.251840	0.008359	0.705532
-44.774530	-1.917385	2.261837	0.008372	0.705535
-44.803432	-1.880846	2.271834	0.008377	0.705599
-43.797754	-1.926357	2.281830	0.008189	0.705868
-43.837426	-1.921251	2.291827	0.008196	0.705865
-43.539191	-1.972953	2.301824	0.008140	0.705869
-43.883981	-1.867898	2.311821	0.008204	0.705958
-43.021655	-1.936324	2.321818	0.008043	0.706130
-43.183679	-1.908792	2.331814	0.008073	0.706128
-43.271061	-1.892542	2.341811	0.008089	0.706130
-42.330632	-1.899408	2.351808	0.007913	0.706454
-42.413306	-1.885629	2.361805	0.007928	0.706453
-42.171881	-1.930896	2.371802	0.007883	0.706449
-41.956184	-1.882300	2.381798	0.007842	0.706625
-41.215410	-1.949781	2.391795	0.007704	0.706756
-41.531874	-1.893326	2.401792	0.007762	0.706757
-41.504235	-1.880771	2.411789	0.007757	0.706793
-40.616459	-1.894471	2.421786	0.007591	0.707084
-40.697499	-1.881102	2.431782	0.007606	0.707082
-40.554004	-1.905880	2.441779	0.007579	0.707085
-39.965565	-1.900427	2.451776	0.007469	0.707307
-39.939582	-1.869031	2.461773	0.007463	0.707380
-39.607745	-1.929709	2.471770	0.007401	0.707378
-39.619465	-1.874534	2.481766	0.007403	0.707485
-38.791854	-1.911207	2.491763	0.007248	0.707709
-38.887662	-1.893883	2.501760	0.007266	0.707710
-38.931543	-1.887370	2.511757	0.007273	0.707708
-38.110501	-1.891777	2.521754	0.007120	0.707994
-38.215000	-1.861019	2.531750	0.007139	0.708019
-37.842319	-1.927493	2.541747	0.007069	0.708020
-37.664870	-1.875420	2.551744	0.007036	0.708188
-37.111210	-1.890094	2.561741	0.006932	0.708357
-37.071116	-1.899522	2.571738	0.006924	0.708354
-37.438321	-1.823425	2.581734	0.006992	0.708376
-36.190155	-1.910428	2.591731	0.006760	0.708648
-36.227941	-1.903794	2.601728	0.006766	0.708649
-36.263872	-1.895814	2.611725	0.006772	0.708653
-35.786925	-1.891255	2.621722	0.006683	0.708833
-35.350653	-1.905688	2.631718	0.006602	0.708960
-35.477932	-1.883146	2.641715	0.006625	0.708961
-35.479496	-1.860996	2.651712	0.006625	0.709006
-34.541838	-1.895188	2.661709	0.006450	0.709273
-34.617641	-1.881663	2.671706	0.006463	0.709273
-34.583107	-1.891390	2.681702	0.006456	0.709267
-33.979458	-1.879018	2.691699	0.006344	0.709508
-33.478855	-1.920783	2.701696	0.006250	0.709604
-33.516235	-1.913948	2.711693	0.006257	0.709605
-33.652979	-1.875737	2.721690	0.006282	0.709633
-32.896675	-1.875295	2.731686	0.006140	0.709905
-32.601972	-1.927474	2.741683	0.006085	0.709906
-32.965871	-1.859334	2.751680	0.006152	0.709913
-32.470640	-1.834287	2.761677	0.006060	0.710141
-31.964921	-1.881138	2.771674	0.005965	0.710228
-32.129871	-1.855053	2.781670	0.005995	0.710222
-31.580586	-1.900315	2.791667	0.005893	0.710328
-30.878418	-1.918480	2.801664	0.005761	0.710543
-30.845853	-1.924928	2.811661	0.005755	0.710542
-31.130682	-1.874865	2.821658	0.005808	0.710542
-30.361548	-1.892680	2.831654	0.005664	0.710781
-30.217816	-1.869981	2.841651	0.005637	0.710878
-30.176386	-1.876952	2.851648	0.005629	0.710880
-29.940878	-1.895568	2.861645	0.005584	0.710927
-29.453899	-1.872828	2.871642	0.005493	0.711147
-29.152412	-1.927072	2.881638	0.005437	0.711146
-29.469047	-1.872127	2.891635	0.005495	0.711144
-29.000853	-1.827754	2.901632	0.005408	0.711400
-28.490702	-1.885411	2.911629	0.005312	0.711467
-28.721143	-1.843710	2.921626	0.005355	0.711469
-28.273906	-1.835504	2.931622	0.005271	0.711646
-27.866864	-1.845037	2.941619	0.005195	0.711772
-27.660298	-1.881387	2.951616	0.005156	0.711774
-27.507126	-1.865432	2.961613	0.005127	0.711861
-26.835074	-1.867822	2.971610	0.005001	0.712096
-26.667926	-1.899031	2.981606	0.004970	0.712093
-26.767043	-1.882137	2.991603	0.004988	0.712093
-26.115456	-1.886722	3.001600	0.004866	0.712316
-25.993901	-1.870275	3.011597	0.004843	0.712393
-26.024095	-1.867151	3.021594	0.004848	0.712389
-25.872976	-1.837373	3.031590	0.004820	0.712503
-25.118606	-1.865378	3.041587	0.004679	0.712715
-24.955708	-1.895750	3.051584	0.004648	0.712714
-24.940573	-1.897053	3.061581	0.004645	0.712717
-24.471551	-1.845258	3.071578	0.004557	0.712987
-24.053552	-1.900504	3.081574	0.004479	0.713027
-24.118662	-1.889434	3.091571	0.004490	0.713026
-24.068461	-1.843705	3.101568	0.004481	0.713136
-23.035177	-1.912569	3.111565	0.004288	0.713366
-23.151631	-1.892550	3.121562	0.004309	0.713365
-23.161607	-1.890753	3.131558	0.004310	0.713366
-22.707481	-1.879391	3.141555	0.004225	0.713551
-22.267388	-1.903700	3.151552	0.004143	0.713659
-22.366331	-1.886408	3.161549	0.004161	0.713659
-22.384288	-1.859100	3.171546	0.004164	0.713708
-21.368049	-1.905520	3.181542	0.003974	0.713976
-21.264400	-1.923884	3.191539	0.003955	0.713977
-21.228772	-1.929580	3.201536	0.003948	0.713979
-21.071540	-1.892732	3.211533	0.003918	0.714109
-20.339986	-1.935284	3.221530	0.003781	0.714284
-20.382366	-1.930703	3.231526	0.003789	0.714279
-20.500288	-1.908418	3.241523	0.003810	0.714283
-19.701093	-1.931401	3.251520	0.003661	0.714521
-19.588515	-1.903901	3.261517	0.003640	0.714616
-19.433963	-1.933926	3.271514	0.003610	0.714612
-19.292795	-1.959050	3.281510	0.003584	0.714613
-18.780474	-1.907372	3.291507	0.003488	0.714897
-18.505069	-1.948492	3.301504	0.003436	0.714914
-18.704748	-1.913180	3.311501	0.003473	0.714914
-18.418538	-1.917562	3.321498	0.003419	0.715007
-17.857626	-1.903640	3.331494	0.003314	0.715234
-17.622140	-1.945995	3.341491	0.003270	0.715234
-17.664538	-1.938736	3.351488	0.003277	0.715234
-17.099006	-1.911335	3.361485	0.003172	0.715489
-16.900780	-1.915885	3.371482	0.003134	0.715551
-16.718811	-1.949613	3.381478	0.003100	0.715549
-16.982651	-1.863587	3.391475	0.003149	0.715628
-15.722011	-1.956718	3.401472	0.002914	0.715889
-15.977075	-1.912450	3.411469	0.002961	0.715888
-15.884696	-1.929512	3.421466	0.002943	0.715887
-15.466206	-1.918976	3.431462	0.002865	0.716057
-15.211650	-1.923711	3.441459	0.002817	0.716138
-14.956521	-1.968536	3.451456	0.002769	0.716140
-15.164707	-1.900633	3.461453	0.002807	0.716202
-14.070144	-1.970970	3.471450	0.002603	0.716449
-14.261441	-1.936523	3.481446	0.002638	0.716451
-14.161110	-1.955356	3.491443	0.002619	0.716450
-13.625855	-1.947900	3.501440	0.002519	0.716654
-13.332926	-1.944826	3.511437	0.002464	0.716764
-13.215037	-1.968088	3.521434	0.002442	0.716761
-13.183899	-1.972387	3.531430	0.002435	0.716764
-12.241771	-1.976408	3.541427	0.002260	0.717089
-12.157467	-1.988950	3.551424	0.002243	0.717095
-12.316313	-1.961468	3.561421	0.002273	0.717094
-12.155777	-1.967680	3.571418	0.002242	0.717139
-11.550093	-1.952903	3.581414	0.002129	0.717382
-11.334660	-1.992154	3.591411	0.002089	0.717382
-11.335322	-1.989761	3.601408	0.002088	0.717387
-10.920993	-1.962400	3.611405	0.002011	0.717588
-10.424459	-1.988547	3.621402	0.001918	0.717712
-10.466645	-1.983620	3.631398	0.001925	0.717707
-10.570937	-1.965301	3.641395	0.001944	0.717708
-9.773213	-1.948669	3.651392	0.001795	0.718022
-9.713210	-1.960675	3.661389	0.001784	0.718020
-9.602436	-1.977965	3.671386	0.001763	0.718026
-9.538302	-1.904325	3.681382	0.001750	0.718195
-8.532075	-2.001512	3.691379	0.001562	0.718358
-8.790559	-1.954470	3.701376	0.001610	0.718360
-8.456909	-2.015917	3.711373	0.001548	0.718357
-7.984104	-1.975032	3.721370	0.001459	0.718605
-7.872808	-1.976342	3.731366	0.001438	0.718642
-7.652628	-2.014021	3.741363	0.001396	0.718646
-7.816029	-1.943494	3.751360	0.001426	0.718729
-6.823157	-2.000650	3.761357	0.001241	0.718966
-6.806049	-2.006246	3.771354	0.001238	0.718962
-6.787193	-2.008312	3.781350	0.001234	0.718965
-6.475563	-1.977831	3.791347	0.001175	0.719135
-6.071384	-1.979061	3.801344	0.001099	0.719276
-5.916037	-2.006381	3.811341	0.001070	0.719277
-5.947947	-2.001863	3.821338	0.001076	0.719276
-5.323553	-1.947883	3.831334	0.000959	0.719602
-5.233351	-1.963047	3.841331	0.000942	0.719605
-5.244015	-1.958785	3.851328	0.000943	0.719610
-4.734736	-1.967457	3.861325	0.000848	0.719773
-4.463961	-1.949187	3.871322	0.000797	0.719905
-4.251891	-1.988112	3.881318	0.000757	0.719903
-4.309400	-1.953299	3.891315	0.000767	0.719952
-3.599201	-1.937480	3.901312	0.000635	0.720233
-3.520404	-1.951762	3.911309	0.000620	0.720234
-3.345762	-1.986522	3.921306	0.000587	0.720227
-3.151936	-1.905495	3.931302	0.000550	0.720456
-2.702928	-1.941516	3.941299	0.000466	0.720543
-2.760066	-1.928936	3.951296	0.000476	0.720549
-2.450640	-1.910165	3.961293	0.000418	0.720695
-2.041082	-1.887563	3.971290	0.000342	0.720884
-2.021226	-1.891628	3.981286	0.000338	0.720883
-2.123730	-1.837928	3.991283	0.000356	0.720954
-1.758963	-1.816730	4.001280	0.000288	0.721124
-1.560895	-1.852007	4.011277	0.000250	0.721125
-1.601436	-1.753462	4.021274	0.000258	0.721305
-1.365945	-1.727724	4.031270	0.000213	0.721439
-1.346118	-1.709766	4.041267	0.000209	0.721482
-1.247775	-1.589741	4.051264	0.000190	0.721754
-1.061938	-1.624112	4.061261	0.000155	0.721752
-1.128055	-1.457850	4.071258	0.000167	0.722056
-1.108804	-1.449437	4.081254	0.000163	0.722080
-0.736119	-1.367947	4.091251	0.000093	0.722371
-0.666561	-1.362037	4.101248	0.000080	0.722408
-0.809361	-1.187955	4.111245	0.000106	0.722701
-0.552581	-1.169972	4.121242	0.000058	0.722827
-0.803336	-1.032314	4.131238	0.000104	0.723010
-0.664539	-0.916644	4.141235	0.000077	0.723286
-0.443180	-0.875881	4.151232	0.000036	0.723444
-0.359486	-0.790025	4.161229	0.000020	0.723643
-0.440669	-0.632081	4.171226	0.000034	0.723925
-0.410608	-0.533499	4.181222	0.000028	0.724129
-0.525860	-0.393818	4.191219	0.000049	0.724363
-0.466442	-0.267625	4.201216	0.000037	0.724632
-0.418782	-0.140206	4.211213	0.000028	0.724899
-0.219743	-0.022900	4.221210	-0.000009	0.725198
-0.113977	0.095883	4.231206	-0.000030	0.725468
0.000000	0.231937	4.241203	-0.000051	0.725775

0.023729	0.845500	4.246208	-0.000056	0.726982
0.375805	2.074048	4.251213	-0.000123	0.729497
0.390370	3.932582	4.256218	-0.000127	0.733108
0.837931	6.278556	4.261222	-0.000212	0.737787
1.359879	9.124039	4.266227	-0.000311	0.743415
1.746975	12.477558	4.271232	-0.000386	0.749917
2.438290	16.234016	4.276237	-0.000517	0.757219
2.945921	20.423249	4.281242	-0.000615	0.765194
3.848866	24.965741	4.286246	-0.000786	0.773863
4.510432	29.919049	4.291251	-0.000913	0.783102
5.231906	35.210654	4.296256	-0.001051	0.792857
5.769856	40.855311	4.301261	-0.001155	0.803060
6.438465	46.776656	4.306266	-0.001283	0.813658
7.198256	52.965664	4.311270	-0.001429	0.824607
7.689240	59.490722	4.316275	-0.001525	0.835902
8.140725	66.204018	4.321280	-0.001614	0.847349
8.888735	73.108610	4.326285	-0.001758	0.859046
9.175040	80.288674	4.331290	-0.001816	0.870901
9.727257	87.601952	4.336294	-0.001924	0.882887
10.293276	95.100055	4.341299	-0.002034	0.895008
10.772357	102.749183	4.346304	-0.002129	0.907179
11.291138	110.558545	4.351309	-0.002230	0.919447
11.913842	118.444303	4.356314	-0.002352	0.931696
12.353549	126.484910	4.361318	-0.002439	0.943971
13.256463	134.554417	4.366323	-0.002613	0.956251
14.640524	142.622390	4.371328	-0.002876	0.968496
15.376553	150.908454	4.376333	-0.003019	0.980738
16.115653	159.276225	4.381338	-0.003162	0.992947
16.555934	167.729125	4.386342	-0.003250	1.005054
17.289980	176.175687	4.391347	-0.003392	1.017079
17.986298	184.667871	4.396352	-0.003527	1.029016
18.525569	193.232259	4.401357	-0.003634	1.040878
19.055518	201.817069	4.406362	-0.003738	1.052631
20.320339	210.308520	4.411366	-0.003979	1.064298
21.391700	218.877271	4.416371	-0.004185	1.075897
21.926793	227.516352	4.421376	-0.004290	1.087342
22.656893	236.148019	4.426381	-0.004432	1.098701
23.610683	244.743589	4.431386	-0.004615	1.109947
24.345910	253.388793	4.436390	-0.004758	1.121094
25.192520	262.013368	4.441395	-0.004921	1.132130
25.900512	270.652684	4.446400	-0.005059	1.143047
26.370841	279.375568	4.451405	-0.005153	1.153914
26.597455	288.060472	4.456410	-0.005201	1.164582
27.405591	296.649975	4.461414	-0.005357	1.175157
28.477166	305.180864	4.466419	-0.005562	1.185622
29.105095	313.792293	4.471424	-0.005685	1.196000
29.879883	322.356445	4.476429	-0.005835	1.206262
30.174286	331.004003	4.481434	-0.005896	1.216440
30.894470	339.558141	4.486438	-0.006036	1.226508
31.532052	348.138870	4.491443	-0.006160	1.236509
32.066410	356.675574	4.496448	-0.006265	1.246359
32.913865	365.185798	4.501453	-0.006429	1.256161
34.016746	373.615047	4.506458	-0.006640	1.265845
34.651642	382.141701	4.511462	-0.006764	1.275475
35.175494	390.647601	4.516467	-0.006867	1.284989
35.514656	399.177441	4.521472	-0.006936	1.294426
36.351007	407.606925	4.526477	-0.007098	1.303775
37.160869	416.134570	4.531482	-0.007254	1.313159
37.953183	424.574616	4.536486	-0.007408	1.322378
38.583003	432.997668	4.541491	-0.007531	1.331487
39.250642	441.396653	4.546496	-0.007661	1.340514
39.703447	449.838003	4.551501	-0.007751	1.349488
39.886057	458.295897	4.556506	-0.007790	1.358372
40.651922	466.635522	4.561510	-0.007939	1.367177
41.667240	474.949901	4.566515	-0.008133	1.375942
42.120528	483.333854	4.571520	-0.008223	1.384626
42.604703	491.740476	4.576525	-0.008319	1.393285
43.024970	500.108102	4.581530	-0.008403	1.401839
43.429360	508.481242	4.586534	-0.008484	1.410345
44.074304	516.807564	4.591539	-0.008610	1.418792
44.498034	525.143830	4.596544	-0.008694	1.427163
45.236619	533.468502	4.601549	-0.008837	1.435524
45.547471	541.798082	4.606554	-0.008901	1.443772
46.016970	550.129417	4.611558	-0.008994	1.452001
46.477170	558.440612	4.616563	-0.009085	1.460162
46.875381	566.753855	4.621568	-0.009165	1.468269
47.545099	575.067890	4.626573	-0.009296	1.476375
48.149080	583.309650	4.631578	-0.009414	1.484358
48.932521	591.549724	4.636582	-0.009565	1.492324
49.024480	599.891071	4.641587	-0.009588	1.500236
49.394214	608.162086	4.646592	-0.009662	1.508083
50.113344	616.407321	4.651597	-0.009802	1.515919
50.417702	624.680529	4.656602	-0.009864	1.523677
50.829223	632.949425	4.661606	-0.009946	1.531408
51.462609	641.182476	4.666611	-0.010070	1.539100
51.804093	649.442976	4.671616	-0.010139	1.546735
52.328647	657.713621	4.676621	-0.010242	1.554369
52.663255	665.949090	4.681626	-0.010310	1.561906
53.091755	674.181809	4.686630	-0.010395	1.569417
53.524625	682.419606	4.691635	-0.010482	1.576898
54.109332	690.604040	4.696640	-0.010596	1.584317
54.663262	698.833057	4.701645	-0.010705	1.591737
54.885129	707.080835	4.706650	-0.010752	1.599092
55.045685	715.328758	4.711654	-0.010787	1.606404
55.478516	723.560760	4.716659	-0.010873	1.613708
56.040517	731.737057	4.721664	-0.010984	1.620947
56.485316	739.953891	4.726669	-0.011072	1.628174
57.030071	748.201387	4.731674	-0.011179	1.635408
57.442467	756.375735	4.736678	-0.011261	1.642530
58.236197	764.518826	4.741683	-0.011415	1.649645
58.894436	772.686302	4.746688	-0.011543	1.656733
59.343463	780.886792	4.751693	-0.011632	1.663789
59.785615	789.072162	4.756698	-0.011720	1.670802
59.989419	797.304671	4.761702	-0.011763	1.677794
60.275737	805.498945	4.766707	-0.011822	1.684735
60.530777	813.694454	4.771712	-0.011875	1.691644
60.826339	821.901106	4.776717	-0.011936	1.698540
61.335906	830.039515	4.781722	-0.012036	1.705379
61.787188	838.234115	4.786726	-0.012126	1.712230
62.078950	846.427998	4.791731	-0.012186	1.719032
62.465129	854.562818	4.796736	-0.012263	1.725771
63.019581	862.725262	4.801741	-0.012372	1.732527
63.112062	870.935176	4.806746	-0.012395	1.739237
63.220529	879.115542	4.811750	-0.012420	1.745899
63.729198	887.276593	4.816755	-0.012521	1.752570
64.095826	895.416978	4.821760	-0.012594	1.759182
64.365702	903.580492	4.826765	-0.012650	1.765775
64.816256	911.728547	4.831770	-0.012740	1.772354
65.366801	919.860054	4.836774	-0.012848	1.778907
65.809598	928.003018	4.841779	-0.012936	1.785432
66.013736	936.216776	4.846784	-0.012979	1.791960
66.533902	944.356498	4.851789	-0.013082	1.798444
66.953399	952.461308	4.856794	-0.013165	1.804866
67.480280	960.587226	4.861798	-0.013269	1.811293
67.860188	968.743358	4.866803	-0.013345	1.817704
68.379735	976.854092	4.871808	-0.013447	1.824074
69.050152	984.989065	4.876813	-0.013578	1.830457
69.354952	993.148292	4.881818	-0.013640	1.836794
69.624543	1001.299350	4.886822	-0.013696	1.843099
69.984256	1009.452563	4.891827	-0.013768	1.849394
70.026145	1017.635275	4.896832	-0.013782	1.855653
70.731835	1025.720472	4.901837	-0.013918	1.861894
70.989790	1033.871090	4.906842	-0.013972	1.868112
71.573423	1042.015833	4.911846	-0.014086	1.874342
72.056419	1050.118334	4.916851	-0.014182	1.880508
72.298418	1058.241248	4.921856	-0.014232	1.886642
72.892552	1066.347834	4.926861	-0.014348	1.892783
73.262071	1074.480178	4.931866	-0.014423	1.898898
73.642202	1082.593168	4.936870	-0.014499	1.904980
74.384770	1090.705266	4.941875	-0.014643	1.911083
74.491123	1098.881682	4.946880	-0.014668	1.917142
75.032334	1106.966783	4.951885	-0.014774	1.923164
75.339587	1115.096783	4.956890	-0.014837	1.929173
75.743692	1123.231675	4.961894	-0.014918	1.935178
76.072809	1131.366872	4.966899	-0.014985	1.941156
76.400005	1139.482014	4.971904	-0.015051	1.947102
76.742606	1147.666475	4.976909	-0.015120	1.953080
77.121296	1155.753208	4.981914	-0.015196	1.958974
77.544688	1163.824814	4.986918	-0.015281	1.964844
78.105626	1171.917370	4.991923	-0.015391	1.970726
78.264371	1180.055721	4.996928	-0.015426	1.976580
78.711321	1188.149902	5.001933	-0.015514	1.982416
79.060944	1196.261307	5.006938	-0.015585	1.988237
79.269580	1204.406281	5.011942	-0.015629	1.994049
79.719935	1212.480076	5.016947	-0.015719	1.999820
79.964501	1220.586142	5.021952	-0.015770	2.005575
80.628060	1228.668879	5.026957	-0.015899	2.011341
80.991829	1236.787589	5.031962	-0.015972	2.017084
81.477592	1244.864932	5.036966	-0.016068	2.022794
82.022576	1252.968658	5.041971	-0.016175	2.028513
82.103208	1261.152754	5.046976	-0.016195	2.034224
82.710202	1269.206182	5.051981	-0.016314	2.039882
82.901018	1277.322732	5.056986	-0.016355	2.045525
83.062151	1285.439523	5.061990	-0.016390	2.051150
83.440328	1293.547468	5.066995	-0.016466	2.056776
83.679476	1301.648189	5.072000	-0.016516	2.062367
84.069069	1309.743238	5.077005	-0.016594	2.067954
84.616016	1317.825020	5.082010	-0.016702	2.073532
85.038147	1325.893736	5.087014	-0.016786	2.079074
85.559334	1333.953164	5.092019	-0.016888	2.084605
85.683562	1342.082302	5.097024	-0.016917	2.090129
86.064650	1350.208118	5.102029	-0.016993	2.095661
86.576261	1358.260138	5.107034	-0.017094	2.101142
86.937684	1366.359004	5.112038	-0.017167	2.106625
87.138793	1374.540128	5.117043	-0.017210	2.112134
87.677945	1382.599505	5.122048	-0.017316	2.117579
88.019677	1390.680350	5.127053	-0.017385	2.123005
88.190472	1398.768665	5.132058	-0.017422	2.128407
88.698769	1406.850689	5.137062	-0.017522	2.133822
89.036479	1414.944573	5.142067	-0.017591	2.139215
89.364413	1423.015608	5.147072	-0.017657	2.144579
89.649228	1431.130347	5.152077	-0.017716	2.149954
90.225043	1439.186795	5.157082	-0.017828	2.155304
90.752029	1447.226573	5.162086	-0.017932	2.160625
91.027717	1455.323757	5.167091	-0.017989	2.165948
91.316524	1463.420775	5.172096	-0.018048	2.171258
91.701799	1471.523686	5.177101	-0.018125	2.176568
92.104139	1479.592040	5.182106	-0.018206	2.181844
92.521635	1487.660240	5.187110	-0.018289	2.187109
92.986958	1495.780148	5.192115	-0.018381	2.192399
93.217637	1503.868021	5.197120	-0.018430	2.197633
93.458225	1511.955986	5.202125	-0.018480	2.202857
93.634070	1520.057340	5.207130	-0.018518	2.208070
94.170184	1528.107123	5.212134	-0.018623	2.213271
94.474184	1536.208552	5.217139	-0.018685	2.218471
94.585081	1544.287827	5.222144	-0.018712	2.223628
95.096666	1552.362373	5.227149	-0.018812	2.228806
95.417095	1560.455664	5.232154	-0.018877	2.233966
95.696252	1568.528957	5.237158	-0.018935	2.239098
96.058966	1576.590038	5.242163	-0.019008	2.244218
96.146198	1584.673614	5.247168	-0.019030	2.249317
96.647014	1592.759715	5.252173	-0.019128	2.254441
97.062538	1600.813090	5.257178	-0.019211	2.259525
97.251786	1608.896757	5.262182	-0.019252	2.264598
97.646591	1616.984548	5.267187	-0.019331	2.269679
97.979346	1625.117145	5.272192	-0.019398	2.274772
98.364754	1633.152038	5.277197	-0.019476	2.279797
98.525637	1641.212911	5.282202	-0.019511	2.284807
98.762139	1649.276408	5.287206	-0.019561	2.289815
99.245363	1657.354758	5.292211	-0.019656	2.294842
99.520562	1665.393409	5.297216	-0.019713	2.299815
99.758296	1673.480987	5.302221	-0.019763	2.304805
100.103704	1681.555751	5.307226	-0.019832	2.309785
100.492122	1689.626998	5.312230	-0.019910	2.314756
100.864829	1697.677320	5.317235	-0.019985	2.319702
101.099261	1705.736975	5.322240	-0.020034	2.324631
101.435411	1713.822196	5.327245	-0.020102	2.329574
101.854619	1721.897076	5.332250	-0.020186	2.334507
102.035610	1729.966884	5.337254	-0.020225	2.339407
102.527373	1738.017909	5.342259	-0.020322	2.344310
102.790225	1746.092436	5.347264	-0.020376	2.349199
103.142305	1754.197654	5.352269	-0.020447	2.354103
103.387318	1762.248805	5.357274	-0.020498	2.358956
104.107718	1770.235029	5.362278	-0.020638	2.363799
104.715825	1778.301827	5.367283	-0.020757	2.368670
104.746691	1786.424826	5.372288	-0.020768	2.373518
105.278047	1794.477235	5.377293	-0.020872	2.378355
105.570709	1802.549127	5.382298	-0.020932	2.383174
105.734321	1810.623434	5.387302	-0.020968	2.387974
106.124594	1818.718749	5.392307	-0.021046	2.392796
106.470931	1826.754485	5.397312	-0.021116	2.397568
107.147104	1834.783045	5.402317	-0.021248	2.402353
107.501740	1842.854276	5.407322	-0.021319	2.407128
107.794729	1850.944627	5.412326	-0.021379	2.411900
108.290498	1859.018770	5.417331	-0.021477	2.416669
108.393059	1867.088465	5.422336	-0.021502	2.421395
109.096476	1875.121239	5.427341	-0.021638	2.426137
109.293448	1883.222967	5.432346	-0.021680	2.430870
109.594922	1891.340590	5.437350	-0.021742	2.435612
110.146547	1899.347117	5.442355	-0.021850	2.440299
110.493099	1907.366343	5.447360	-0.021920	2.444968
110.863984	1915.420661	5.452365	-0.021995	2.449651
111.009363	1923.525002	5.457370	-0.022027	2.454337
111.500145	1931.537959	5.462374	-0.022124	2.458986
111.895032	1939.598762	5.467379	-0.022203	2.463648
111.952975	1947.687620	5.472384	-0.022219	2.468291
112.359792	1955.767982	5.477389	-0.022300	2.472947
112.653528	1963.813431	5.482394	-0.022361	2.477565
112.770141	1971.876489	5.487398	-0.022388	2.482172
113.359878	1979.903562	5.492403	-0.022503	2.486785
113.621373	1987.965222	5.497408	-0.022557	2.491384
113.942134	1996.047538	5.502413	-0.022622	2.495991
114.407433	2004.080844	5.507418	-0.022714	2.500573
114.734736	2012.124530	5.512422	-0.022781	2.505141
115.486817	2020.164600	5.517427	-0.022926	2.509730
115.824669	2028.270746	5.522432	-0.022995	2.514318
116.184283	2036.296820	5.527437	-0.023067	2.518853
116.458195	2044.347434	5.532442	-0.023124	2.523389
116.742894	2052.396266	5.537446	-0.023182	2.527915
117.310724	2060.469495	5.542451	-0.023293	2.532468
117.543556	2068.527967	5.547456	-0.023342	2.536980
117.886912	2076.595883	5.552461	-0.023412	2.541497
118.397896	2084.608215	5.557466	-0.023512	2.545987
119.004902	2092.648765	5.562470	-0.023631	2.550491
119.342990	2100.766115	5.567475	-0.023699	2.555011
119.498157	2108.809528	5.572480	-0.023733	2.559469
120.010294	2116.836526	5.577485	-0.023834	2.563935
120.612988	2124.885452	5.582490	-0.023952	2.568412
120.788347	2132.957030	5.587494	-0.023990	2.572864
121.247683	2141.013636	5.592499	-0.024081	2.577319
121.467701	2149.065697	5.597504	-0.024127	2.581747
121.786759	2157.129339	5.602509	-0.024192	2.586181
122.018155	2165.235129	5.607514	-0.024241	2.590625
122.335960	2173.451093	5.612518	-0.024306	2.595126
122.959106	2181.401292	5.617523	-0.024427	2.599496
123.125707	2189.407881	5.622528	-0.024464	2.603859
123.583284	2197.416971	5.627533	-0.024554	2.608234
123.857068	2205.466594	5.632538	-0.024611	2.612612
123.880803	2213.542316	5.637542	-0.024620	2.616980
124.293617	2221.574844	5.642547	-0.024703	2.621344
124.693299	2229.586680	5.647552	-0.024783	2.625688
124.836354	2237.658711	5.652557	-0.024815	2.630040
124.903146	2245.756775	5.657562	-0.024833	2.634393
125.291304	2253.756320	5.662566	-0.024910	2.638708
125.852666	2261.769003	5.667571	-0.025020	2.643035
126.145704	2269.815683	5.672576	-0.025080	2.647354
126.323189	2277.904728	5.677581	-0.025119	2.651682
126.653259	2285.962405	5.682586	-0.025186	2.655995
126.952314	2293.988983	5.687590	-0.025247	2.660283
127.365156	2302.020761	5.692595	-0.025329	2.664575
127.662429	2310.062662	5.697600	-0.025390	2.668857
127.932752	2318.161662	5.702605	-0.025446	2.673160
128.255179	2326.213774	5.707610	-0.025511	2.677436
128.848085	2334.184717	5.712614	-0.025627	2.681678
129.317081	2342.232212	5.717619	-0.025720	2.685947
129.368907	2350.320987	5.722624	-0.025735	2.690204
129.683469	2358.382137	5.727629	-0.025799	2.694456
130.344120	2366.399224	5.732634	-0.025928	2.698700
130.598235	2374.424852	5.737638	-0.025980	2.702916
130.955044	2382.507700	5.742643	-0.026052	2.707162
131.301393	2390.554997	5.747648	-0.026122	2.711382
131.579476	2398.652562	5.752653	-0.026180	2.715617
131.823343	2406.660674	5.757658	-0.026230	2.719798
132.195983	2414.681613	5.762662	-0.026305	2.723986
132.685117	2422.731446	5.767667	-0.026402	2.728189
132.926316	2430.805817	5.772672	-0.026452	2.732384
133.374031	2438.840546	5.777677	-0.026541	2.736565
133.839058	2446.876706	5.782682	-0.026633	2.740740
134.240688	2454.874652	5.787686	-0.026713	2.744886
134.493185	2462.977146	5.792691	-0.026766	2.749070
134.689742	2471.092619	5.797696	-0.026808	2.753251
135.079122	2479.124874	5.802701	-0.026886	2.757395
135.494717	2487.118794	5.807706	-0.026969	2.761514
135.675038	2495.153579	5.812710	-0.027008	2.765634
136.147827	2503.191461	5.817715	-0.027101	2.769766
136.759063	2511.213877	5.822720	-0.027220	2.773893
137.215296	2519.251255	5.827725	-0.027311	2.778012
137.687070	2527.257233	5.832730	-0.027404	2.782109
137.846498	2535.348371	5.837734	-0.027439	2.786226
138.021052	2543.421471	5.842739	-0.027477	2.790328
138.361550	2551.467662	5.847744	-0.027546	2.794420
138.603833	2559.509335	5.852749	-0.027597	2.798498
138.822645	2567.564961	5.857754	-0.027643	2.802575
139.055419	2575.580005	5.862758	-0.027692	2.806627
139.680578	2583.613980	5.867763	-0.027813	2.810706
139.903724	2591.670512	5.872768	-0.027861	2.814766
140.038371	2599.719642	5.877773	-0.027891	2.818812
140.552386	2607.730327	5.882778	-0.027992	2.822854
140.865230	2615.773177	5.887782	-0.028056	2.826895
141.223954	2623.851280	5.892787	-0.028128	2.830951
141.367039	2631.918645	5.897792	-0.028160	2.834983
141.924088	2639.906199	5.902797	-0.028269	2.838993
142.333335	2647.943417	5.907802	-0.028351	2.843013
142.734149	2655.953570	5.912806	-0.028431	2.847014
143.354574	2663.992702	5.917811	-0.028552	2.851036
143.732611	2672.039867	5.922816	-0.028628	2.855042
143.931375	2680.097187	5.927821	-0.028670	2.859038
144.231579	2688.169719	5.932826	-0.028732	2.863042
144.594488	2696.182732	5.937830	-0.028805	2.867013
144.874758	2704.254349	5.942835	-0.028863	2.871004
145.220959	2712.280463	5.947840	-0.028932	2.874970
145.785325	2720.303141	5.952845	-0.029043	2.878941
146.151313	2728.338211	5.957850	-0.029117	2.882902
146.436144	2736.368016	5.962854	-0.029175	2.886850
146.854658	2744.440823	5.967859	-0.029258	2.890821
147.161096	2752.472734	5.972864	-0.029321	2.894760
147.403569	2760.531138	5.977869	-0.029372	2.898703
147.807035	2768.547024	5.982874	-0.029452	2.902629
148.203865	2776.572792	5.987878	-0.029531	2.906554
148.605518	2784.668919	5.992883	-0.029612	2.910508
148.699854	2792.790589	5.997888	-0.029635	2.914453
149.272540	2800.745315	6.002893	-0.029747	2.918337
149.376779	2808.784629	6.007898	-0.029772	2.922231
149.315069	2816.830161	6.012902	-0.029766	2.926115
149.714346	2824.864120	6.017907	-0.029845	2.930012
150.117062	2832.873614	6.022912	-0.029926	2.933893
150.184216	2840.939347	6.027917	-0.029944	2.937777
150.655992	2848.948679	6.032922	-0.030037	2.941651
151.099975	2856.941883	6.037926	-0.030125	2.945510
151.586764	2864.999219	6.042931	-0.030221	2.949397
151.835745	2873.065594	6.047936	-0.030273	2.953271
152.392599	2881.078965	6.052941	-0.030382	2.957130
152.968636	2889.090585	6.057946	-0.030495	2.960984
153.222242	2897.096957	6.062950	-0.030548	2.964814
153.505746	2905.191340	6.067955	-0.030606	2.968682
153.785824	2913.235706	6.072960	-0.030664	2.972522
153.990222	2921.296699	6.077965	-0.030707	2.976360
154.387445	2929.314828	6.082970	-0.030786	2.980183
154.548778	2937.374380	6.087974	-0.030822	2.984009
155.039045	2945.403666	6.092979	-0.030919	2.987832
154.807927	2953.511659	6.097984	-0.030881	2.991651
155.118827	2961.529799	6.102989	-0.030945	2.995450
155.502275	2969.524148	6.107994	-0.031021	2.999236
155.640037	2977.536658	6.112998	-0.031052	3.003014
156.050402	2985.572669	6.118003	-0.031134	3.006812
156.219731	2993.611643	6.123008	-0.031171	3.010594
156.363660	3001.696120	6.128013	-0.031204	3.014392
156.999446	3009.680300	6.133018	-0.031327	3.018161
157.382086	3017.695762	6.138022	-0.031404	3.021929
157.790228	3025.749555	6.143027	-0.031485	3.025710
158.118477	3033.777050	6.148032	-0.031552	3.029471
158.566788	3041.832467	6.153037	-0.031641	3.033246
158.967825	3049.894981	6.158042	-0.031721	3.037017
159.184914	3057.889200	6.163046	-0.031767	3.040743
159.669394	3065.898855	6.168051	-0.031863	3.044484
159.691772	3073.976779	6.173056	-0.031872	3.048230
159.940603	3082.022597	6.178061	-0.031924	3.051967
160.480037	3090.046710	6.183066	-0.032030	3.055704
160.816434	3098.036701	6.188070	-0.032098	3.059410
161.028395	3106.100008	6.193075	-0.032143	3.063140
161.264158	3114.136945	6.198080	-0.032192	3.066854
161.760628	3122.171590	6.203085	-0.032290	3.070575
161.989426	3130.330993	6.208090	-0.032338	3.074336
162.395981	3138.287956	6.213094	-0.032419	3.078008
162.678408	3146.319601	6.218099	-0.032477	3.081704
163.017697	3154.291888	6.223104	-0.032546	3.085371
163.117882	3162.329249	6.228109	-0.032570	3.089052
163.219040	3170.425388	6.233114	-0.032595	3.092755
163.448081	3178.463060	6.238118	-0.032643	3.096434
164.021800	3186.429422	6.243123	-0.032755	3.100091
164.330795	3194.438026	6.248128	-0.032818	3.103751
164.721808	3202.497563	6.253133	-0.032896	3.107433
165.120417	3210.568867	6.258138	-0.032976	3.111117
165.363150	3218.560702	6.263142	-0.033026	3.114753
165.630734	3226.615398	6.268147	-0.033082	3.118415
165.979419	3234.635126	6.273152	-0.033152	3.122059
166.033557	3242.662291	6.278157	-0.033168	3.125690
166.361737	3250.705820	6.283162	-0.033234	3.129337
166.582554	3258.746566	6.288166	-0.033281	3.132972
166.810190	3266.803735	6.293171	-0.033329	3.136612
167.024355	3274.839761	6.298176	-0.033374	3.140237
167.454975	3282.833520	6.303181	-0.033460	3.143848
167.833349	3290.870308	6.308186	-0.033535	3.147472
168.019511	3298.909424	6.313190	-0.033576	3.151084
168.600495	3306.955918	6.318195	-0.033689	3.154713
168.684256	3314.988783	6.323200	-0.033710	3.158310
169.106470	3322.992631	6.328205	-0.033794	3.161904
169.302595	3331.018460	6.333210	-0.033836	3.165495
169.548861	3339.029773	6.338214	-0.033888	3.169077
169.991652	3347.112829	6.343219	-0.033975	3.172695
170.115102	3355.153704	6.348224	-0.034004	3.176276
170.408810	3363.150914	6.353229	-0.034064	3.179842
170.730400	3371.217250	6.358234	-0.034129	3.183435
170.929698	3379.223445	6.363238	-0.034172	3.186992
171.235989	3387.293454	6.368243	-0.034234	3.190578
171.658834	3395.307992	6.373248	-0.034319	3.194140
171.882344	3403.346279	6.378253	-0.034366	3.197700
172.109417	3411.399679	6.383258	-0.034413	3.201263
172.255831	3419.369123	6.388262	-0.034446	3.204782
172.755906	3427.425603	6.393267	-0.034545	3.208350
173.058280	3435.439506	6.398272	-0.034606	3.211887
173.411731	3443.459759	6.403277	-0.034678	3.215425
173.774905	3451.527988	6.408282	-0.034751	3.218980
174.222993	3459.489811	6.413286	-0.034840	3.222488
174.651670	3467.540821	6.418291	-0.034925	3.226031
175.125877	3475.581683	6.423296	-0.035019	3.229567
175.418823	3483.680539	6.428301	-0.035079	3.233117
175.839661	3491.740858	6.433306	-0.035162	3.236651
176.061682	3499.669426	6.438310	-0.035209	3.240116
176.643249	3507.680450	6.443315	-0.035323	3.243628
176.447628	3515.751595	6.448320	-0.035292	3.247131
176.504702	3523.774460	6.453325	-0.035308	3.250619
176.900000	3531.822603	6.458330	-0.035387	3.254128
177.110981	3539.840227	6.463334	-0.035432	3.257612
177.635732	3547.852451	6.468339	-0.035535	3.261103
177.779201	3555.866229	6.473344	-0.035567	3.264576
178.141590	3563.911450	6.478349	-0.035640	3.268067
178.247856	3571.989313	6.483354	-0.035665	3.271558
178.579314	3580.001970	6.488358	-0.035732	3.275026
179.089637	3588.008659	6.493363	-0.035833	3.278495
179.366797	3596.021774	6.498368	-0.035890	3.281954
179.592201	3604.039398	6.503373	-0.035937	3.285409
179.825295	3612.090353	6.508378	-0.035986	3.288875
179.998052	3620.153115	6.513382	-0.036024	3.292340
180.154223	3628.212817	6.518387	-0.036058	3.295800
180.453966	3636.185139	6.523392	-0.036120	3.299224
180.848860	3644.240021	6.528397	-0.036199	3.302683
181.030824	3652.280674	6.533402	-0.036238	3.306124
180.997511	3660.293138	6.538406	-0.036237	3.309542
181.350346	3668.377381	6.543411	-0.036308	3.313001
181.575040	3676.403004	6.548416	-0.036356	3.316427
181.793727	3684.352383	6.553421	-0.036402	3.319817
182.221679	3692.378461	6.558426	-0.036487	3.323243
182.351946	3700.410282	6.563430	-0.036517	3.326657
182.665551	3708.411648	6.568435	-0.036580	3.330062
182.806815	3716.490142	6.573440	-0.036612	3.333489
183.184418	3724.522613	6.578445	-0.036688	3.336902
183.435558	3732.533780	6.583450	-0.036740	3.340298
183.637495	3740.556728	6.588454	-0.036783	3.343693
184.059044	3748.589786	6.593459	-0.036867	3.347098
184.194382	3756.620949	6.598464	-0.036898	3.350487
184.160660	3764.686656	6.603469	-0.036897	3.353882
184.503746	3772.734294	6.608474	-0.036966	3.357279
184.597347	3780.710401	6.613478	-0.036989	3.360633
184.833771	3788.734483	6.618483	-0.037039	3.364010
184.979964	3796.759501	6.623488	-0.037071	3.367380
185.203177	3804.800287	6.628493	-0.037118	3.370756
185.467029	3812.865974	6.633498	-0.037173	3.374141
185.806521	3820.847597	6.638502	-0.037242	3.377489
186.185420	3828.887851	6.643507	-0.037318	3.380860
186.256421	3836.909716	6.648512	-0.037336	3.384210
186.500538	3844.932589	6.653517	-0.037387	3.387562
186.650767	3853.009624	6.658522	-0.037421	3.390930
187.161913	3861.076750	6.663526	-0.037521	3.394304
187.494650	3869.083527	6.668531	-0.037589	3.397642
187.411298	3877.073367	6.673536	-0.037579	3.400956
187.521765	3885.066251	6.678541	-0.037605	3.404275
187.902990	3893.096692	6.683546	-0.037681	3.407615
188.083950	3901.106392	6.688550	-0.037720	3.410937
188.367531	3909.171472	6.693555	-0.037778	3.414281
188.603978	3917.196287	6.698560	-0.037828	3.417605
188.592753	3925.211411	6.703565	-0.037831	3.420912
188.831177	3933.225324	6.708570	-0.037881	3.424224
188.931610	3941.218136	6.713574	-0.037905	3.427520
189.173017	3949.285453	6.718579	-0.037956	3.430847
189.407528	3957.343046	6.723584	-0.038005	3.434168
189.442860	3965.365300	6.728589	-0.038017	3.437464
189.863949	3973.361190	6.733594	-0.038101	3.440758
189.886249	3981.364196	6.738598	-0.038110	3.444039
190.158212	3989.432659	6.743603	-0.038166	3.447353
190.466553	3997.433583	6.748608	-0.038229	3.450636
190.476611	4005.543234	6.753613	-0.038237	3.453951
190.868301	4013.521731	6.758618	-0.038315	3.457221
191.031828	4021.542144	6.763622	-0.038351	3.460499
191.326371	4029.529226	6.768627	-0.038411	3.463763
191.257019	4037.617137	6.773632	-0.038404	3.467054
191.578386	4045.609012	6.778637	-0.038469	3.470315
191.794490	4053.697527	6.783642	-0.038515	3.473609
191.829023	4061.693419	6.788646	-0.038526	3.476857
192.408479	4069.671186	6.793651	-0.038640	3.480111
192.554818	4077.688132	6.798656	-0.038672	3.483365
192.781294	4085.721079	6.803661	-0.038720	3.486624
192.868118	4093.777116	6.808666	-0.038742	3.489885
193.128183	4101.787147	6.813670	-0.038796	3.493130
193.339708	4109.840219	6.818675	-0.038840	3.496388
193.518691	4117.830619	6.823680	-0.038879	3.499617
193.874319	4125.842837	6.828685	-0.038951	3.502856
194.095187	4133.910200	6.833690	-0.038997	3.506111
194.015931	4141.931202	6.838694	-0.038988	3.509335
194.284744	4149.960251	6.843699	-0.039044	3.512570
194.563638	4158.002292	6.848704	-0.039101	3.515807
194.771119	4165.983313	6.853709	-0.039145	3.519014
194.916392	4174.027862	6.858714	-0.039178	3.522242
194.971437	4182.001630	6.863718	-0.039193	3.525437
195.414998	4190.051847	6.868723	-0.039281	3.528670
195.479009	4198.095128	6.873728	-0.039299	3.531886
195.619652	4206.118926	6.878733	-0.039330	3.535094
196.220415	4214.128300	6.883738	-0.039448	3.538307
196.430246	4222.160208	6.888742	-0.039492	3.541514
196.692172	4230.165827	6.893747	-0.039546	3.544710
196.967136	4238.226514	6.898752	-0.039603	3.547924
197.169475	4246.273285	6.903757	-0.039646	3.551129
197.392890	4254.421052	6.908762	-0.039693	3.554370
197.432526	4262.381219	6.913766	-0.039706	3.557530
197.670942	4270.344970	6.918771	-0.039756	3.560693
197.795290	4278.331344	6.923776	-0.039784	3.563859
197.745000	4286.373913	6.928781	-0.039780	3.567040
198.247732	4294.385861	6.933786	-0.039879	3.570222
198.338222	4302.420019	6.938790	-0.039902	3.573397
198.643692	4310.492550	6.943795	-0.039964	3.576592
198.962418	4318.430469	6.948800	-0.040029	3.579730
199.048964	4326.487337	6.953805	-0.040050	3.582906
199.137206	4334.549692	6.958810	-0.040072	3.586082
199.421284	4342.502780	6.963814	-0.040131	3.589217
199.740093	4350.563048	6.968819	-0.040195	3.592392
199.946042	4358.614744	6.973824	-0.040239	3.595558
199.953818	4366.594489	6.978829	-0.040246	3.598688
200.472525	4374.623221	6.983834	-0.040348	3.601848
200.750949	4382.563673	6.988838	-0.040405	3.604964
200.664026	4390.664566	6.993843	-0.040395	3.608130
200.800360	4398.699355	6.998848	-0.040426	3.611273
201.192893	4406.706518	7.003853	-0.040504	3.614410
201.468864	4414.752963	7.008858	-0.040561	3.617557
201.486320	4422.770010	7.013862	-0.040570	3.620682
201.859510	4430.775775	7.018867	-0.040645	3.623809
201.913714	4438.813876	7.023872	-0.040660	3.626938
202.029033	4446.872418	7.028877	-0.040687	3.630074
202.713361	4454.910169	7.033882	-0.040820	3.633214
202.665156	4462.948209	7.038886	-0.040816	3.636332
202.769512	4470.939215	7.043891	-0.040841	3.639433
202.960760	4478.947301	7.048896	-0.040882	3.642540
203.165266	4486.962226	7.053901	-0.040926	3.645648
203.481877	4494.999114	7.058906	-0.040990	3.648764
203.746295	4503.030380	7.063910	-0.041045	3.651875
204.032156	4511.072840	7.068915	-0.041104	3.654987
204.218109	4519.096606	7.073920	-0.041144	3.658087
204.219927	4527.124192	7.078925	-0.041149	3.661181
204.471025	4535.143569	7.083930	-0.041202	3.664275
204.541604	4543.159123	7.088934	-0.041220	3.667361
204.828764	4551.197166	7.093939	-0.041279	3.670458
204.974003	4559.251519	7.098944	-0.041312	3.673556
205.315481	4567.242022	7.103949	-0.041381	3.676631
205.373896	4575.252278	7.108954	-0.041397	3.679704
205.392548	4583.245783	7.113958	-0.041406	3.682767
205.754676	4591.279815	7.118963	-0.041479	3.685851
205.938836	4599.314374	7.123968	-0.041518	3.688929
206.274721	4607.331169	7.128973	-0.041586	3.692001
206.523865	4615.354689	7.133978	-0.041638	3.695071
206.738106	4623.343046	7.138982	-0.041684	3.698124
206.874615	4631.384077	7.143987	-0.041714	3.701193
207.042165	4639.388857	7.148992	-0.041751	3.704246
207.275023	4647.424870	7.153997	-0.041800	3.707310
207.590086	4655.447617	7.159002	-0.041864	3.710368
207.675421	4663.543524	7.164006	-0.041885	3.713446
208.124131	4671.608360	7.169011	-0.041974	3.716518
208.285451	4679.551659	7.174016	-0.042010	3.719535
208.535614	4687.531328	7.179021	-0.042062	3.722565
208.806336	4695.550142	7.184026	-0.042118	3.725608
209.122170	4703.547228	7.189030	-0.042182	3.728642
209.192053	4711.604320	7.194035	-0.042200	3.731689
209.273805	4719.616037	7.199040	-0.042221	3.734718
209.544562	4727.639961	7.204045	-0.042277	3.737752
209.933805	4735.673978	7.209050	-0.042355	3.740791
209.931213	4743.651817	7.214054	-0.042360	3.743798
210.329580	4751.691087	7.219059	-0.042439	3.746834
210.432158	4759.755997	7.224064	-0.042464	3.749870
210.429989	4767.792345	7.229069	-0.042469	3.752891
210.732823	4775.843235	7.234074	-0.042531	3.755922
211.012345	4783.833109	7.239078	-0.042588	3.758927
211.168490	4791.870278	7.244083	-0.042623	3.761944
211.424470	4799.819606	7.249088	-0.042676	3.764929
211.864718	4807.861905	7.254093	-0.042763	3.767949
212.216497	4815.926173	7.259098	-0.042834	3.770974
212.418000	4823.945878	7.264102	-0.042877	3.773976
212.456597	4831.996799	7.269107	-0.042890	3.776984
212.639158	4839.987051	7.274112	-0.042929	3.779970
213.089721	4847.986311	7.279117	-0.043019	3.782963
213.292387	4856.010891	7.284122	-0.043062	3.785957
213.381646	4864.048571	7.289126	-0.043084	3.788951
213.506627	4872.097285	7.294131	-0.043113	3.791948
213.821545	4880.131281	7.299136	-0.043177	3.794941
214.131532	4888.099733	7.304141	-0.043240	3.797907
214.352969	4896.127651	7.309146	-0.043287	3.800891
214.275154	4904.115228	7.314150	-0.043278	3.803852
214.469461	4912.170067	7.319155	-0.043319	3.806840
214.869702	4920.160484	7.324160	-0.043399	3.809807
214.989157	4928.208797	7.329165	-0.043427	3.812787
215.054887	4936.262298	7.334170	-0.043445	3.815765
215.264027	4944.218449	7.339174	-0.043489	3.818709
215.453107	4952.284363	7.344179	-0.043530	3.821689
215.663140	4960.269950	7.349184	-0.043574	3.824639
215.847720	4968.281873	7.354189	-0.043614	3.827595
216.042474	4976.343617	7.359194	-0.043656	3.830567
216.026904	4984.369104	7.364198	-0.043658	3.833520
216.388942	4992.413801	7.369203	-0.043731	3.836485
216.651301	5000.381980	7.374208	-0.043785	3.839417
217.042033	5008.402050	7.379213	-0.043863	3.842369
217.377942	5016.411891	7.384218	-0.043931	3.845314
217.597454	5024.436099	7.389222	-0.043978	3.848259
217.910669	5032.485329	7.394227	-0.044042	3.851213
218.028728	5040.513077	7.399232	-0.044069	3.854153
217.924611	5048.567581	7.404237	-0.044055	3.857096
218.601182	5056.523697	7.409242	-0.044186	3.860017
218.796668	5064.571016	7.414246	-0.044228	3.862959
218.928570	5072.610843	7.419251	-0.044258	3.865894
219.019560	5080.655602	7.424256	-0.044281	3.868829
219.181089	5088.689049	7.429261	-0.044316	3.871758
219.124402	5096.957305	7.434266	-0.044311	3.874766
219.685841	5104.820662	7.439270	-0.044421	3.877637
219.743470	5112.756100	7.444275	-0.044437	3.880522
220.049134	5120.739532	7.449280	-0.044500	3.883427
220.172961	5128.743729	7.454285	-0.044528	3.886334
220.393239	5136.788589	7.459290	-0.044575	3.889255
220.494594	5144.806107	7.464294	-0.044599	3.892162
220.625719	5152.813470	7.469299	-0.044629	3.895064
220.972638	5160.836499	7.474304	-0.044699	3.897973
221.104697	5168.823977	7.479309	-0.044729	3.900863
221.609399	5176.857236	7.484314	-0.044828	3.903774
221.794459	5184.881802	7.489318	-0.044868	3.906674
221.983313	5192.877591	7.494323	-0.044909	3.909562
222.168445	5200.948889	7.499328	-0.044949	3.912474
222.297710	5208.978798	7.504333	-0.044978	3.915369
222.604562	5216.997156	7.509338	-0.045041	3.918260
222.672153	5224.960541	7.514342	-0.045059	3.921125
222.885420	5232.965146	7.519347	-0.045104	3.924005
223.178551	5241.056150	7.524352	-0.045164	3.926916
223.244478	5249.023471	7.529357	-0.045182	3.929776
223.526832	5257.094900	7.534362	-0.045240	3.932675
223.616192	5265.073750	7.539366	-0.045262	3.935535
223.893671	5273.100769	7.544371	-0.045319	3.938414
224.035547	5281.120277	7.549376	-0.045351	3.941286
224.174489	5289.095176	7.554381	-0.045382	3.944139
224.460263	5297.162407	7.559386	-0.045441	3.947026
224.681729	5305.152138	7.564390	-0.045487	3.949882
224.767757	5313.252264	7.569395	-0.045509	3.952773
224.993225	5321.258877	7.574400	-0.045556	3.955631
225.279624	5329.244832	7.579405	-0.045615	3.958481
225.477234	5337.276823	7.584410	-0.045657	3.961343
225.514596	5345.208954	7.589414	-0.045670	3.964165
225.710533	5353.292253	7.594419	-0.045712	3.967041
225.973799	5361.278139	7.599424	-0.045766	3.969882
225.886331	5369.321290	7.604429	-0.045755	3.972735
226.414918	5377.371754	7.609434	-0.045859	3.975599
226.523780	5385.369960	7.614438	-0.045885	3.978435
226.467743	5393.377932	7.619443	-0.045880	3.981270
226.749685	5401.409760	7.624448	-0.045938	3.984117
226.991536	5409.413950	7.629453	-0.045988	3.986952
227.227457	5417.472823	7.634458	-0.046038	3.989803
227.363709	5425.534968	7.639462	-0.046068	3.992652
227.662128	5433.582415	7.644467	-0.046129	3.995497
227.698184	5441.596036	7.649472	-0.046142	3.998323
227.631042	5449.572946	7.654477	-0.046134	4.001133
227.955585	5457.566551	7.659482	-0.046200	4.003953
228.323457	5465.583560	7.664486	-0.046274	4.006780
228.210733	5473.597202	7.669491	-0.046259	4.009596
228.642139	5481.680755	7.674496	-0.046345	4.012443
228.755817	5489.672820	7.679501	-0.046371	4.015250
228.916373	5497.714799	7.684506	-0.046406	4.018075
228.896487	5505.715923	7.689510	-0.046408	4.020880
229.295500	5513.727909	7.694515	-0.046488	4.023693
229.442795	5521.778685	7.699520	-0.046521	4.026514
229.597503	5529.762563	7.704525	-0.046555	4.029310
230.114004	5537.815418	7.709530	-0.046657	4.032133
230.193730	5545.912127	7.714534	-0.046677	4.034963
230.289642	5553.875240	7.719539	-0.046700	4.037745
230.514128	5561.855557	7.724544	-0.046748	4.040532
230.803309	5569.810149	7.729549	-0.046807	4.043310
231.120349	5577.829249	7.734554	-0.046871	4.046109
231.159192	5585.847498	7.739558	-0.046884	4.048901
231.365208	5593.887830	7.744563	-0.046928	4.051701
231.713091	5601.904710	7.749568	-0.046998	4.054494
231.777060	5609.922553	7.754573	-0.047015	4.057280
231.976546	5617.919810	7.759578	-0.047058	4.060060
232.202058	5625.951303	7.764582	-0.047105	4.062850
232.516443	5633.950655	7.769587	-0.047169	4.065628
232.727408	5641.984049	7.774592	-0.047214	4.068414
232.943116	5649.994899	7.779597	-0.047260	4.071191
233.127259	5658.086566	7.784602	-0.047299	4.073993
233.245483	5666.112397	7.789606	-0.047327	4.076770
233.312315	5674.068020	7.794611	-0.047345	4.079520
233.568371	5682.100430	7.799616	-0.047398	4.082297
233.616392	5690.064053	7.804621	-0.047412	4.085045
233.759445	5698.129061	7.809626	-0.047444	4.087828
233.952569	5706.132475	7.814630	-0.047486	4.090589
233.954680	5714.203930	7.819635	-0.047492	4.093368
234.241804	5722.252008	7.824640	-0.047550	4.096142
234.402477	5730.193248	7.829645	-0.047586	4.098875
234.820294	5738.252065	7.834650	-0.047669	4.101649
234.797798	5746.205512	7.839654	-0.047670	4.104381
234.993665	5754.263592	7.844659	-0.047712	4.107148
235.121764	5762.282328	7.849664	-0.047741	4.109900
234.995020	5770.356792	7.854669	-0.047723	4.112666
235.379675	5778.391668	7.859674	-0.047800	4.115423
235.820421	5786.381718	7.864678	-0.047888	4.118163
236.058432	5794.390027	7.869683	-0.047938	4.120905
235.967988	5802.430107	7.874688	-0.047926	4.123652
236.304604	5810.410090	7.879693	-0.047994	4.126382
236.422547	5818.411449	7.884698	-0.048022	4.129115
236.385080	5826.480378	7.889702	-0.048020	4.131867
236.604530	5834.499914	7.894707	-0.048067	4.134603
237.016254	5842.525530	7.899712	-0.048149	4.137342
237.113118	5850.463836	7.904717	-0.048172	4.140046
237.316294	5858.529495	7.909722	-0.048215	4.142792
237.498201	5866.526920	7.914726	-0.048255	4.145513
237.521594	5874.558034	7.919731	-0.048264	4.148242
237.807863	5882.566282	7.924736	-0.048323	4.150965
238.119899	5890.645321	7.929741	-0.048387	4.153709
238.191804	5898.708364	7.934746	-0.048406	4.156444
238.383329	5906.629944	7.939750	-0.048447	4.159131
238.501057	5914.647694	7.944755	-0.048474	4.161847
238.830908	5922.659188	7.949760	-0.048541	4.164562
238.941687	5930.671171	7.954765	-0.048567	4.167273
239.107759	5938.686638	7.959770	-0.048603	4.169984
239.250568	5946.776569	7.964774	-0.048635	4.172718
239.554398	5954.782535	7.969779	-0.048697	4.175423
239.688962	5962.788085	7.974784	-0.048728	4.178125
239.732099	5970.761926	7.979789	-0.048741	4.180813
239.979337	5978.768831	7.984794	-0.048793	4.183513
240.001051	5986.845556	7.989798	-0.048802	4.186233
240.398584	5994.838876	7.994803	-0.048882	4.188926
240.532172	6002.883710	7.999808	-0.048912	4.191632
240.700594	6011.006172	8.004813	-0.048949	4.194363
240.871281	6019.005584	8.009818	-0.048986	4.197051
240.987573	6026.909465	8.014822	-0.049013	4.199704
241.242869	6034.912021	8.019827	-0.049066	4.202390
241.375722	6042.919726	8.024832	-0.049096	4.205075
241.381211	6050.939174	8.029837	-0.049103	4.207761
241.426592	6058.990578	8.034842	-0.049117	4.210456
241.591618	6067.020335	8.039846	-0.049153	4.213144
241.708472	6075.010911	8.044851	-0.049180	4.215816
242.051861	6083.016920	8.049856	-0.049249	4.218493
242.051848	6091.028626	8.054861	-0.049255	4.221168
242.218715	6099.026643	8.059866	-0.049291	4.223838
242.299260	6107.106228	8.064870	-0.049312	4.226533
242.747787	6115.043867	8.069875	-0.049401	4.229182
242.760377	6123.115088	8.074880	-0.049409	4.231869
242.828364	6131.167401	8.079885	-0.049427	4.234550
243.151723	6139.215037	8.084890	-0.049492	4.237229
243.376665	6147.147489	8.089894	-0.049540	4.239867
243.417192	6155.208434	8.094899	-0.049553	4.242545
243.853188	6163.185802	8.099904	-0.049639	4.245197
243.871522	6171.172871	8.104909	-0.049648	4.247847
243.973433	6179.225851	8.109914	-0.049673	4.250517
244.100349	6187.290831	8.114918	-0.049702	4.253190
244.408644	6195.323211	8.119923	-0.049765	4.255852
244.558819	6203.307265	8.124928	-0.049798	4.258495
244.638353	6211.279271	8.129933	-0.049818	4.261132
244.787953	6219.337634	8.134938	-0.049851	4.263797
244.978430	6227.326318	8.139942	-0.049892	4.266437
245.062904	6235.369053	8.144947	-0.049914	4.269092
245.066745	6243.454820	8.149952	-0.049920	4.271759
245.480421	6251.461652	8.154957	-0.050002	4.274402
245.806139	6259.508946	8.159962	-0.050068	4.277055
245.920535	6267.423271	8.164966	-0.050095	4.279662
246.230024	6275.496290	8.169971	-0.050158	4.282321
246.236849	6283.493356	8.174976	-0.050165	4.284950
246.229330	6291.501388	8.179981	-0.050169	4.287582
246.433833	6299.547404	8.184986	-0.050212	4.290226
246.645104	6307.583093	8.189990	-0.050257	4.292865
246.781631	6315.574134	8.194995	-0.050288	4.295487
247.133020	6323.622365	8.200000	-0.050359	4.298128
247.450447	6331.545868	8.205005	-0.050423	4.300726
247.605754	6339.590501	8.210010	-0.050458	4.303361
247.557960	6347.616030	8.215014	-0.050454	4.305987
247.689603	6355.662537	8.220019	-0.050484	4.308619
247.892938	6363.690477	8.225024	-0.050528	4.311244
247.875045	6371.698559	8.230029	-0.050530	4.313859
248.216767	6379.784138	8.235034	-0.050599	4.316501
248.310428	6387.731709	8.240038	-0.050622	4.319094
248.660087	6395.697855	8.245043	-0.050692	4.321693
248.805503	6403.724023	8.250048	-0.050725	4.324309
248.887694	6411.752591	8.255053	-0.050745	4.326924
249.133347	6419.755830	8.260058	-0.050797	4.329530
249.380261	6427.825432	8.265062	-0.050848	4.332156
249.616588	6435.798397	8.270067	-0.050897	4.334748
249.949057	6443.870471	8.275072	-0.050965	4.337372
249.763804	6451.842347	8.280077	-0.050936	4.339959
250.006043	6459.877942	8.285082	-0.050986	4.342567
250.229579	6467.830221	8.290086	-0.051033	4.345147
250.277349	6475.880323	8.295091	-0.051048	4.347756
250.403943	6483.917398	8.300096	-0.051077	4.350359
250.672078	6491.994327	8.305101	-0.051132	4.352975
250.869101	6500.051480	8.310106	-0.051174	4.355582
250.856643	6508.011122	8.315110	-0.051177	4.358155
251.341419	6515.988671	8.320115	-0.051273	4.360735
251.491960	6523.965547	8.325120	-0.051306	4.363311
251.564205	6531.998926	8.330125	-0.051325	4.365904
251.901568	6540.019867	8.335130	-0.051394	4.368492
251.969571	6548.037794	8.340134	-0.051412	4.371077
252.145087	6556.042172	8.345139	-0.051450	4.373656
252.437299	6564.133776	8.350144	-0.051510	4.376262
252.626900	6572.043726	8.355149	-0.051550	4.378808
252.801120	6580.141227	8.360154	-0.051588	4.381412
252.824052	6588.094489	8.365158	-0.051598	4.383968
253.024270	6596.114691	8.370163	-0.051641	4.386544
253.385979	6604.193551	8.375168	-0.051714	4.389139
253.416088	6612.169646	8.380173	-0.051725	4.391698
253.737316	6620.242313	8.385178	-0.051790	4.394287
253.846240	6628.252968	8.390182	-0.051816	4.396854
254.017372	6636.214740	8.395187	-0.051853	4.399404
254.154624	6644.283213	8.400192	-0.051884	4.401986
254.170873	6652.192276	8.405197	-0.051892	4.404516
254.346000	6660.307783	8.410202	-0.051930	4.407111
254.519712	6668.251217	8.415206	-0.051968	4.409649
254.787824	6676.304588	8.420211	-0.052023	4.412221
255.032121	6684.380726	8.425216	-0.052074	4.414799
255.110504	6692.389556	8.430221	-0.052094	4.417353
255.373446	6700.408382	8.435226	-0.052149	4.419909
255.516639	6708.433574	8.440230	-0.052181	4.422466
255.709221	6716.359807	8.445235	-0.052222	4.424990
255.854234	6724.478767	8.450240	-0.052255	4.427573
256.044474	6732.437922	8.455245	-0.052296	4.430105
256.286096	6740.529809	8.460250	-0.052346	4.432677
256.501541	6748.518656	8.465254	-0.052392	4.435215
256.797916	6756.506260	8.470259	-0.052452	4.437751
257.081273	6764.515455	8.475264	-0.052510	4.440293
257.165643	6772.565215	8.480269	-0.052532	4.442845
257.312676	6780.526263	8.485274	-0.052564	4.445368
257.565791	6788.560704	8.490278	-0.052617	4.447913
257.583529	6796.553173	8.495283	-0.052626	4.450442
257.718099	6804.631846	8.500288	-0.052656	4.452998
257.865693	6812.627155	8.505293	-0.052689	4.455526
258.259933	6820.662985	8.510298	-0.052768	4.458066
258.284941	6828.652052	8.515302	-0.052778	4.460589
258.297575	6836.650736	8.520307	-0.052786	4.463113
258.783199	6844.663043	8.525312	-0.052882	4.465641
258.834509	6852.697277	8.530317	-0.052897	4.468174
259.008730	6860.734904	8.535322	-0.052935	4.470706
259.250812	6868.747756	8.540326	-0.052985	4.473230
259.336491	6876.737913	8.545331	-0.053006	4.475744
259.615783	6884.778505	8.550336	-0.053064	4.478274
259.570940	6892.739220	8.555341	-0.053061	4.480776
260.046870	6900.751523	8.560346	-0.053155	4.483294
260.123370	6908.781884	8.565351	-0.053175	4.485815
260.288664	6916.810090	8.570355	-0.053211	4.488335
260.571767	6924.846901	8.575360	-0.053269	4.490856
260.673585	6932.866872	8.580365	-0.053294	4.493370
260.714340	6940.907807	8.585370	-0.053307	4.495888
260.951610	6948.895931	8.590375	-0.053356	4.498390
261.090028	6956.885337	8.595379	-0.053387	4.500890
261.284382	6964.911804	8.600384	-0.053429	4.503400
261.493133	6972.926747	8.605389	-0.053473	4.505906
261.820980	6980.949436	8.610394	-0.053540	4.508412
261.879947	6988.996500	8.615399	-0.053556	4.510925
262.131056	6997.027841	8.620403	-0.053608	4.513431
262.504253	7005.057994	8.625408	-0.053683	4.515936
262.479519	7013.021991	8.630413	-0.053684	4.518418
262.671254	7021.018188	8.635418	-0.053725	4.520909
262.976870	7028.985141	8.640423	-0.053788	4.523390
262.982911	7037.026460	8.645427	-0.053794	4.525891
263.176909	7045.072269	8.650432	-0.053836	4.528394
263.100898	7053.060659	8.655437	-0.053827	4.530876
263.434322	7061.121819	8.660442	-0.053895	4.533381
263.281799	7069.121411	8.665447	-0.053872	4.535864
263.419310	7077.123050	8.670451	-0.053903	4.538347
263.820298	7085.162264	8.675456	-0.053983	4.540841
263.996735	7093.150540	8.680461	-0.054021	4.543317
264.334968	7101.184975	8.685466	-0.054089	4.545806
264.470087	7109.211579	8.690471	-0.054120	4.548291
264.626178	7117.204210	8.695475	-0.054155	4.550764
264.646835	7125.261275	8.700480	-0.054164	4.553256
264.600389	7133.253258	8.705485	-0.054161	4.555726
264.972287	7141.287809	8.710490	-0.054235	4.558208
265.140118	7149.264721	8.715495	-0.054272	4.560671
265.245693	7157.244147	8.720499	-0.054297	4.563134
265.416930	7165.273351	8.725504	-0.054334	4.565610
265.567040	7173.328310	8.730509	-0.054368	4.568093
265.748791	7181.317715	8.735514	-0.054407	4.570554
265.968964	7189.392583	8.740519	-0.054454	4.573041
266.075631	7197.419337	8.745523	-0.054479	4.575511
266.294831	7205.450337	8.750528	-0.054525	4.577981
266.373837	7213.393470	8.755533	-0.054545	4.580423
266.668590	7221.462668	8.760538	-0.054606	4.582902
266.916172	7229.423504	8.765543	-0.054657	4.585346
266.915417	7237.430531	8.770547	-0.054662	4.587804
267.191539	7245.500831	8.775552	-0.054719	4.590279
267.374961	7253.476803	8.780557	-0.054759	4.592724
267.457991	7261.565130	8.785562	-0.054780	4.595202
267.256065	7269.630242	8.790567	-0.054748	4.597672
267.604198	7277.545833	8.795571	-0.054818	4.600095
267.817861	7285.594274	8.800576	-0.054863	4.602557
267.765955	7293.522266	8.805581	-0.054859	4.604981
267.986658	7301.625387	8.810586	-0.054905	4.607457
268.135672	7309.604034	8.815591	-0.054939	4.609894
268.268300	7317.623774	8.820595	-0.054969	4.612342
268.583929	7325.671686	8.825600	-0.055033	4.614797
268.632925	7333.700983	8.830605	-0.055048	4.617245
268.884587	7341.626374	8.835610	-0.055100	4.619660
268.993154	7349.694099	8.840615	-0.055125	4.622118
269.062753	7357.637849	8.845619	-0.055144	4.624536
269.172553	7365.757296	8.850624	-0.055170	4.627006
269.248737	7373.750625	8.855629	-0.055189	4.629437
269.374756	7381.787387	8.860634	-0.055218	4.631880
269.576762	7389.790662	8.865639	-0.055261	4.634311
269.809871	7397.814791	8.870643	-0.055310	4.636747
270.076978	7405.818666	8.875648	-0.055365	4.639176
270.291788	7413.809143	8.880653	-0.055411	4.641599
270.396777	7421.783871	8.885658	-0.055436	4.644016
270.286139	7429.829914	8.890663	-0.055421	4.646454
270.621667	7437.843972	8.895667	-0.055489	4.648881
271.110629	7445.898149	8.900672	-0.055585	4.651318
271.071012	7453.877803	8.905677	-0.055583	4.653732
271.267945	7461.908228	8.910682	-0.055625	4.656159
271.421499	7469.914801	8.915687	-0.055659	4.658578
271.416818	7477.890627	8.920691	-0.055664	4.660987
271.528173	7485.955030	8.925696	-0.055690	4.663422
271.727610	7493.928987	8.930701	-0.055732	4.665827
271.979050	7502.007909	8.935706	-0.055785	4.668263
271.910724	7509.963802	8.940711	-0.055777	4.670661
272.494286	7518.040934	8.945715	-0.055892	4.673093
272.664930	7526.157126	8.950720	-0.055929	4.675536
272.529375	7534.129233	8.955725	-0.055909	4.677936
272.728121	7542.023627	8.960730	-0.055951	4.680309
273.235536	7550.074960	8.965735	-0.056051	4.682729
273.180254	7557.994508	8.970739	-0.056046	4.685108
273.187614	7566.107804	8.975744	-0.056053	4.687545
273.140230	7574.076125	8.980749	-0.056050	4.689937
273.265144	7582.166466	8.985754	-0.056079	4.692363
273.474624	7590.145094	8.990759	-0.056123	4.694755
273.431878	7598.165367	8.995763	-0.056121	4.697159
273.612990	7606.172891	9.000768	-0.056160	4.699557
273.927120	7614.177404	9.005773	-0.056224	4.701952
274.036859	7622.149857	9.010778	-0.056249	4.704337
274.093100	7630.272105	9.015783	-0.056265	4.706766
274.109904	7638.262396	9.020787	-0.056274	4.709155
274.305716	7646.231289	9.025792	-0.056316	4.711535
274.560989	7654.278081	9.030797	-0.056369	4.713937
274.971544	7662.323304	9.035802	-0.056451	4.716337
274.979708	7670.281823	9.040807	-0.056458	4.718711
275.064222	7678.282857	9.045811	-0.056479	4.721096
275.363270	7686.322723	9.050816	-0.056540	4.723491
275.424791	7694.313920	9.055821	-0.056557	4.725871
275.586034	7702.361667	9.060826	-0.056592	4.728266
275.793500	7710.399386	9.065831	-0.056636	4.730657
275.820325	7718.445518	9.070835	-0.056647	4.733049
275.985635	7726.476321	9.075840	-0.056683	4.735436
276.121235	7734.447831	9.080845	-0.056714	4.737804
276.461134	7742.440545	9.085850	-0.056783	4.740176
276.499367	7750.475840	9.090855	-0.056795	4.742560
276.569358	7758.427162	9.095859	-0.056814	4.744919
277.028299	7766.510569	9.100864	-0.056904	4.747314
277.148186	7774.457998	9.105869	-0.056932	4.749668
277.190937	7782.542333	9.110874	-0.056946	4.752062
277.484241	7790.621391	9.115879	-0.057006	4.754453
277.643696	7798.618426	9.120883	-0.057041	4.756819
277.755563	7806.589303	9.125888	-0.057067	4.759175
277.780855	7814.541869	9.130893	-0.057077	4.761526
278.029055	7822.573351	9.135898	-0.057129	4.763898
278.134518	7830.584723	9.140903	-0.057154	4.766263
278.484654	7838.571872	9.145907	-0.057225	4.768619
278.650369	7846.629256	9.150912	-0.057261	4.770995
278.710873	7854.641526	9.155917	-0.057278	4.773357
278.868668	7862.723881	9.160922	-0.057312	4.775738
278.860004	7870.670010	9.165927	-0.057316	4.778079
279.140246	7878.678541	9.170931	-0.057374	4.780435
279.393638	7886.723623	9.175936	-0.057426	4.782801
279.285006	7894.705552	9.180941	-0.057412	4.785149
279.694963	7902.742071	9.185946	-0.057493	4.787510
279.987360	7910.743639	9.190951	-0.057553	4.789860
280.147497	7918.777948	9.195955	-0.057589	4.792218
280.326063	7926.809141	9.200960	-0.057627	4.794575
280.440226	7934.827326	9.205965	-0.057654	4.796927
280.553817	7942.769618	9.210970	-0.057681	4.799255
280.836410	7950.884907	9.215975	-0.057739	4.801632
280.751951	7958.816797	9.220979	-0.057728	4.803956
280.892140	7966.884396	9.225984	-0.057760	4.806318
281.006327	7974.865937	9.230989	-0.057787	4.808653
281.220605	7982.880948	9.235994	-0.057832	4.810996
281.340308	7990.304406	9.240999	-0.057859	4.813166
281.522088	7994.745016	9.246003	-0.057896	4.814463

281.606580	7997.288369	9.251008	-0.057914	4.815206
281.786558	7998.598511	9.256013	-0.057948	4.815587
281.849944	7999.103007	9.261018	-0.057961	4.815734
281.937109	8000.043978	9.266023	-0.057978	4.816009
282.104484	8000.044912	9.271027	-0.058009	4.816008
282.093357	8000.063967	9.276032	-0.058007	4.816014
282.244067	8000.073148	9.281037	-0.058036	4.816016
282.287725	8000.008773	9.286042	-0.058044	4.815997
282.208443	8000.076815	9.291047	-0.058029	4.816017
282.384133	8000.052253	9.296051	-0.058062	4.816009
282.359302	8000.094570	9.301056	-0.058058	4.816021
282.706505	8000.049622	9.306061	-0.058123	4.816006
282.504933	8000.034212	9.311066	-0.058085	4.816003
282.717567	8000.053072	9.316071	-0.058125	4.816007
282.674021	7999.993519	9.321075	-0.058117	4.815990
282.590240	8000.066823	9.326080	-0.058102	4.816012
282.607777	8000.025484	9.331085	-0.058105	4.816000
282.668037	8000.053322	9.336090	-0.058117	4.816008
282.850803	8000.087668	9.341095	-0.058151	4.816017
282.561393	7999.980884	9.346099	-0.058097	4.815987
282.854123	8000.087771	9.351104	-0.058152	4.816017
283.032256	8000.031191	9.356109	-0.058186	4.815999
283.012750	8000.011619	9.361114	-0.058182	4.815994
282.817889	8000.144885	9.366119	-0.058146	4.816034
283.079009	8000.083406	9.371123	-0.058195	4.816014
283.180252	8000.086342	9.376128	-0.058214	4.816015
283.104970	8000.081784	9.381133	-0.058200	4.816014
283.125658	8000.068289	9.386138	-0.058204	4.816010
283.367659	8000.117610	9.391143	-0.058250	4.816023
283.299517	7999.966765	9.396147	-0.058237	4.815979
283.294274	8000.041502	9.401152	-0.058236	4.816001
283.423738	8000.065259	9.406157	-0.058261	4.816007
283.242180	8000.080137	9.411162	-0.058227	4.816012
283.374870	8000.065478	9.416167	-0.058252	4.816007
283.302571	8000.024638	9.421171	-0.058239	4.815996
283.396912	8000.060579	9.426176	-0.058256	4.816006
283.442352	8000.048604	9.431181	-0.058265	4.816002
283.463744	8000.058634	9.436186	-0.058269	4.816005
283.502522	8000.093562	9.441191	-0.058277	4.816015
283.564769	8000.070137	9.446195	-0.058289	4.816008
283.526399	8000.126102	9.451200	-0.058282	4.816024
283.545234	8000.117916	9.456205	-0.058285	4.816022
283.612937	8000.077491	9.461210	-0.058298	4.816010
283.399898	8000.127064	9.466215	-0.058259	4.816025
283.433692	8000.059302	9.471219	-0.058265	4.816005
283.490296	8000.121274	9.476224	-0.058276	4.816023
283.227214	8000.104741	9.481229	-0.058227	4.816020
283.373806	8000.025142	9.486234	-0.058255	4.815995
283.493121	8000.126732	9.491239	-0.058277	4.816025
283.586336	8000.072879	9.496243	-0.058295	4.816008
283.713764	8000.079499	9.501248	-0.058319	4.816010
283.652980	8000.101924	9.506253	-0.058308	4.816016
283.696901	8000.127327	9.511258	-0.058316	4.816024
283.909932	8000.085278	9.516263	-0.058356	4.816010
283.718419	8000.107456	9.521267	-0.058320	4.816018
283.920676	8000.134679	9.526272	-0.058358	4.816025
283.690980	8000.108066	9.531277	-0.058316	4.816018
283.765535	8000.078453	9.536282	-0.058330	4.816009
284.063036	8000.087107	9.541287	-0.058385	4.816010
284.089393	8000.025621	9.546291	-0.058391	4.815992
283.833572	8000.038076	9.551296	-0.058343	4.815997
284.017970	8000.017948	9.556301	-0.058378	4.815990
283.969240	8000.024561	9.561306	-0.058369	4.815992
283.695534	8000.124328	9.566311	-0.058318	4.816023
283.606731	8000.090667	9.571315	-0.058302	4.816013
283.968750	8000.138973	9.576320	-0.058369	4.816025
284.067668	8000.102323	9.581325	-0.058388	4.816014
283.746134	8000.124267	9.586330	-0.058328	4.816022
283.888936	8000.139718	9.591335	-0.058355	4.816026
284.141427	8000.111213	9.596339	-0.058402	4.816016
284.023074	8000.144344	9.601344	-0.058381	4.816027
283.945188	8000.150426	9.606349	-0.058366	4.816029
284.200418	8000.132659	9.611354	-0.058414	4.816022
284.368596	8000.120786	9.616359	-0.058446	4.816018
284.298434	8000.105633	9.621363	-0.058433	4.816014
284.423587	8000.111144	9.626368	-0.058456	4.816015
284.389168	8000.063511	9.631373	-0.058450	4.816001
284.234061	8000.036121	9.636378	-0.058421	4.815994
284.418366	8000.102561	9.641383	-0.058456	4.816012
284.395807	8000.079727	9.646387	-0.058452	4.816006
284.336441	8000.093628	9.651392	-0.058441	4.816010
284.244566	8000.129379	9.656397	-0.058424	4.816021
284.324668	8000.079561	9.661402	-0.058439	4.816006
284.329918	8000.157698	9.666407	-0.058441	4.816029
284.222572	8000.115147	9.671411	-0.058421	4.816017
284.354820	8000.129338	9.676416	-0.058446	4.816020
284.297281	8000.115484	9.681421	-0.058435	4.816017
284.429477	8000.092266	9.686426	-0.058460	4.816009
284.574576	8000.139823	9.691431	-0.058487	4.816022
284.347926	8000.088683	9.696435	-0.058445	4.816009
284.392008	8000.127984	9.701440	-0.058454	4.816020
284.576668	8000.070454	9.706445	-0.058488	4.816002
284.523043	8000.090873	9.711450	-0.058478	4.816008
284.509881	8000.145161	9.716455	-0.058476	4.816024
284.332567	8000.077821	9.721459	-0.058443	4.816005
284.490364	8000.097821	9.726464	-0.058473	4.816010
284.260032	8000.080815	9.731469	-0.058430	4.816007
284.077468	8000.068955	9.736474	-0.058397	4.816004
284.411213	8000.059033	9.741479	-0.058459	4.816000
284.551024	8000.045574	9.746483	-0.058485	4.815995
284.469890	8000.171299	9.751488	-0.058470	4.816032
284.283429	8000.142267	9.756493	-0.058436	4.816025
284.522410	8000.073972	9.761498	-0.058480	4.816003
284.569961	8000.095167	9.766503	-0.058490	4.816009
284.249852	8000.016672	9.771507	-0.058430	4.815988
284.642361	8000.104012	9.776512	-0.058503	4.816011
284.575028	8000.103873	9.781517	-0.058491	4.816012
284.331934	8000.102665	9.786522	-0.058446	4.816013
284.523117	8000.045254	9.791527	-0.058482	4.815995
284.683717	8000.020417	9.796531	-0.058512	4.815987
284.642229	8000.106252	9.801536	-0.058505	4.816012
284.615258	8000.138913	9.806541	-0.058500	4.816022
284.766476	8000.114974	9.811546	-0.058528	4.816014
284.740089	8000.145509	9.816551	-0.058523	4.816023
284.595771	8000.089457	9.821555	-0.058497	4.816007
284.735452	8000.135847	9.826560	-0.058523	4.816020
284.657707	8000.131243	9.831565	-0.058509	4.816019
284.582254	8000.168364	9.836570	-0.058495	4.816030
284.586261	8000.129982	9.841575	-0.058496	4.816019
284.591175	8000.124749	9.846579	-0.058497	4.816018
284.735399	8000.138089	9.851584	-0.058524	4.816021
284.674316	8000.118827	9.856589	-0.058513	4.816015
284.763272	8000.106577	9.861594	-0.058530	4.816011
284.981176	8000.169358	9.866599	-0.058570	4.816029
284.667153	8000.178611	9.871603	-0.058512	4.816033
284.738168	8000.164965	9.876608	-0.058526	4.816029
284.926327	8000.163076	9.881613	-0.058561	4.816027
284.737906	8000.073087	9.886618	-0.058526	4.816002
284.890831	8000.152851	9.891623	-0.058555	4.816024
284.764652	8000.123850	9.896627	-0.058531	4.816016
284.921810	8000.109638	9.901632	-0.058561	4.816011
284.725514	8000.083633	9.906637	-0.058525	4.816005
284.760124	8000.097111	9.911642	-0.058531	4.816009
284.908985	8000.140463	9.916647	-0.058559	4.816020
284.829545	8000.073838	9.921651	-0.058545	4.816001
285.088982	8000.126689	9.926656	-0.058593	4.816015
284.927487	8000.090631	9.931661	-0.058563	4.816006
284.770348	8000.030070	9.936666	-0.058534	4.815989
284.939268	8000.173184	9.941671	-0.058566	4.816030
284.927868	8000.105664	9.946675	-0.058564	4.816010
285.282354	8000.150631	9.951680	-0.058630	4.816021
284.919231	8000.138681	9.956685	-0.058563	4.816020
285.043859	8000.091812	9.961690	-0.058586	4.816005
285.141876	8000.133167	9.966695	-0.058605	4.816017
284.935061	8000.118726	9.971699	-0.058566	4.816014
284.918407	8000.107755	9.976704	-0.058564	4.816011
285.003374	8000.127496	9.981709	-0.058580	4.816016
284.780530	8000.119176	9.986714	-0.058538	4.816015
284.709384	8000.138205	9.991719	-0.058525	4.816021
284.952709	8000.115947	9.996723	-0.058571	4.816013
285.027280	8000.134430	10.001728	-0.058585	4.816018
285.020645	8000.127917	10.006733	-0.058584	4.816016
285.208419	8000.123884	10.011738	-0.058619	4.816014
285.310413	8000.173862	10.016743	-0.058638	4.816028
284.939731	8000.151086	10.021747	-0.058569	4.816023
285.153001	8000.182788	10.026752	-0.058609	4.816031
285.043660	8000.163713	10.031757	-0.058589	4.816026
285.205391	8000.100420	10.036762	-0.058620	4.816007
285.283966	8000.142490	10.041767	-0.058634	4.816019
285.117587	8000.064659	10.046771	-0.058604	4.815997
285.141778	8000.158106	10.051776	-0.058608	4.816024
285.165613	8000.151081	10.056781	-0.058613	4.816022
285.026269	8000.096188	10.061786	-0.058587	4.816007
285.114226	8000.122397	10.066791	-0.058604	4.816014
285.133259	8000.065051	10.071795	-0.058608	4.815997
285.101427	8000.146788	10.076800	-0.058602	4.816021
285.257132	8000.120793	10.081805	-0.058631	4.816013
285.248506	8000.114244	10.086810	-0.058630	4.816011
285.290140	8000.119300	10.091815	-0.058638	4.816012
285.235834	8000.109780	10.096819	-0.058628	4.816010
285.343405	8000.131003	10.101824	-0.058648	4.816015
285.083257	8000.129482	10.106829	-0.058600	4.816016
284.949456	8000.130268	10.111834	-0.058575	4.816017
285.092830	8000.161763	10.116839	-0.058602	4.816025
285.112025	8000.088387	10.121843	-0.058606	4.816004
285.236597	8000.109920	10.126848	-0.058629	4.816010
285.178687	8000.119572	10.131853	-0.058619	4.816013
285.302624	8000.113305	10.136858	-0.058642	4.816010
285.114479	8000.123787	10.141863	-0.058607	4.816014
285.193728	8000.093190	10.146867	-0.058622	4.816005
285.067789	8000.122977	10.151872	-0.058599	4.816014
285.026369	8000.129724	10.156877	-0.058591	4.816016
285.068616	8000.086695	10.161882	-0.058599	4.816004
285.107462	8000.087425	10.166887	-0.058607	4.816004
285.109011	8000.055411	10.171891	-0.058607	4.815994
285.119718	8000.109067	10.176896	-0.058610	4.816010
285.209475	8000.189817	10.181901	-0.058627	4.816033
285.073833	8000.125372	10.186906	-0.058601	4.816015
285.135530	8000.184235	10.191911	-0.058613	4.816032
285.004337	8000.135903	10.196915	-0.058589	4.816018
285.178219	8000.118791	10.201920	-0.058622	4.816012
285.157392	8000.132326	10.206925	-0.058618	4.816016
285.064757	8000.123175	10.211930	-0.058601	4.816014
285.184491	8000.164927	10.216935	-0.058623	4.816026
285.307151	8000.044275	10.221939	-0.058646	4.815990
285.262878	8000.072345	10.226944	-0.058638	4.815998
285.230106	8000.115589	10.231949	-0.058633	4.816011
285.243265	8000.127607	10.236954	-0.058635	4.816015
285.261920	8000.110868	10.241959	-0.058639	4.816010
285.081017	8000.050942	10.246963	-0.058605	4.815993
285.081579	8000.143958	10.251968	-0.058606	4.816020
285.179771	8000.127601	10.256973	-0.058624	4.816015
285.177267	8000.115820	10.261978	-0.058624	4.816011
285.369884	8000.142870	10.266983	-0.058660	4.816018
285.074060	8000.102222	10.271987	-0.058605	4.816008
285.264016	8000.170907	10.276992	-0.058641	4.816027
285.289625	8000.143606	10.281997	-0.058646	4.816019
285.195231	8000.187863	10.287002	-0.058628	4.816032
285.420866	8000.174902	10.292007	-0.058671	4.816027
285.355778	8000.139533	10.297011	-0.058659	4.816017
285.384011	8000.178547	10.302016	-0.058664	4.816029
285.047837	8000.161744	10.307021	-0.058602	4.816025
284.925045	8000.190519	10.312026	-0.058579	4.816035
285.293673	8000.206887	10.317031	-0.058648	4.816037
285.321775	8000.156119	10.322035	-0.058653	4.816022
285.349046	8000.185495	10.327040	-0.058659	4.816031
285.359011	8000.166460	10.332045	-0.058661	4.816025
285.274456	8000.146768	10.337050	-0.058645	4.816020
285.397749	8000.174691	10.342055	-0.058669	4.816027
285.256358	8000.165718	10.347059	-0.058642	4.816025
285.135831	8000.191328	10.352064	-0.058620	4.816034
285.299844	8000.156935	10.357069	-0.058651	4.816023
285.378086	8000.151972	10.362074	-0.058666	4.816021
285.576032	8000.183395	10.367079	-0.058703	4.816029
285.472843	8000.128092	10.372083	-0.058684	4.816013
285.311711	8000.115553	10.377088	-0.058654	4.816010
285.353783	8000.160163	10.382093	-0.058662	4.816023
285.494095	8000.123199	10.387098	-0.058688	4.816012
285.549689	8000.174469	10.392103	-0.058699	4.816026
285.423608	8000.117680	10.397107	-0.058676	4.816010
285.415629	8000.135725	10.402112	-0.058674	4.816016
285.612732	8000.123312	10.407117	-0.058711	4.816011
285.341103	8000.131200	10.412122	-0.058661	4.816015
285.417204	8000.198877	10.417127	-0.058675	4.816034
285.279324	8000.115152	10.422131	-0.058650	4.816010
285.574100	8000.153687	10.427136	-0.058705	4.816020
285.400030	8000.169769	10.432141	-0.058673	4.816026
285.361091	8000.148772	10.437146	-0.058666	4.816020
285.394641	8000.172919	10.442151	-0.058672	4.816027
285.296714	8000.178634	10.447155	-0.058654	4.816029
285.348157	8000.165700	10.452160	-0.058664	4.816025
285.366453	8000.169261	10.457165	-0.058668	4.816026
285.339792	8000.120700	10.462170	-0.058663	4.816012
285.542903	8000.181075	10.467175	-0.058701	4.816028
285.478627	8000.055941	10.472179	-0.058689	4.815992
285.401624	8000.131511	10.477184	-0.058675	4.816015
285.338617	8000.100455	10.482189	-0.058663	4.816006
285.343755	8000.061025	10.487194	-0.058665	4.815994
285.600026	8000.135196	10.492199	-0.058713	4.816015
285.552479	8000.065945	10.497203	-0.058704	4.815995
285.549346	8000.114006	10.502208	-0.058704	4.816009
285.637521	8000.160526	10.507213	-0.058720	4.816022
285.562396	8000.133524	10.512218	-0.058706	4.816014
285.578342	8000.142387	10.517223	-0.058710	4.816017
285.708843	8000.072112	10.522227	-0.058734	4.815995
285.696077	8000.110377	10.527232	-0.058732	4.816007
285.459346	8000.132797	10.532237	-0.058688	4.816015
285.552894	8000.043677	10.537242	-0.058706	4.815988
285.700587	8000.113729	10.542247	-0.058733	4.816008
285.488420	8000.123771	10.547251	-0.058694	4.816012
285.532591	8000.114980	10.552256	-0.058703	4.816009
285.603797	8000.159053	10.557261	-0.058716	4.816021
285.364858	8000.146162	10.562266	-0.058672	4.816019
285.477586	8000.205956	10.567271	-0.058693	4.816036
285.544656	8000.121697	10.572275	-0.058706	4.816011
285.627595	8000.129645	10.577280	-0.058721	4.816013
285.523542	8000.149143	10.582285	-0.058702	4.816019
285.538971	8000.125932	10.587290	-0.058705	4.816012
285.576942	8000.182224	10.592295	-0.058713	4.816028
285.527849	8000.127909	10.597299	-0.058704	4.816013
285.586570	8000.108694	10.602304	-0.058715	4.816007
285.671017	8000.082468	10.607309	-0.058731	4.815999
285.520315	8000.031642	10.612314	-0.058703	4.815985
285.598669	8000.106841	10.617319	-0.058718	4.816006
285.440834	8000.043059	10.622323	-0.058689	4.815988
285.590095	8000.114208	10.627328	-0.058717	4.816008
285.407261	8000.141887	10.632333	-0.058683	4.816017
285.331564	8000.106325	10.637338	-0.058669	4.816007
285.568206	8000.122423	10.642343	-0.058713	4.816011
285.589133	8000.092899	10.647347	-0.058717	4.816002
285.656077	8000.112312	10.652352	-0.058730	4.816007
285.697037	8000.122700	10.657357	-0.058738	4.816010
285.675769	8000.135159	10.662362	-0.058734	4.816014
285.590623	8000.194548	10.667367	-0.058718	4.816032
285.571383	8000.129020	10.672371	-0.058715	4.816013
285.764681	8000.118675	10.677376	-0.058751	4.816009
285.756036	8000.139915	10.682381	-0.058750	4.816015
285.633005	8000.087456	10.687386	-0.058727	4.816000
285.653985	8000.170158	10.692391	-0.058731	4.816024
285.452266	8000.061754	10.697395	-0.058694	4.815994
285.466487	8000.121888	10.702400	-0.058697	4.816011
285.700659	8000.117633	10.707405	-0.058741	4.816009
285.646649	8000.083535	10.712410	-0.058731	4.815999
285.695536	8000.127201	10.717415	-0.058740	4.816011
285.502201	8000.101248	10.722419	-0.058704	4.816005
285.638644	8000.106966	10.727424	-0.058730	4.816006
285.557086	8000.106567	10.732429	-0.058715	4.816006
285.629666	8000.102569	10.737434	-0.058729	4.816005
285.880353	8000.192672	10.742439	-0.058776	4.816030
285.879937	8000.168103	10.747443	-0.058776	4.816022
285.706946	8000.183136	10.752448	-0.058744	4.816028
285.777564	8000.140625	10.757453	-0.058757	4.816015
285.699648	8000.117847	10.762458	-0.058743	4.816009
285.767074	8000.149026	10.767463	-0.058756	4.816017
285.790936	8000.127037	10.772467	-0.058760	4.816011
285.786931	8000.102403	10.777472	-0.058760	4.816004
285.718569	8000.171718	10.782477	-0.058747	4.816024
285.853291	8000.115413	10.787482	-0.058772	4.816007
285.992672	8000.120117	10.792487	-0.058799	4.816008
285.759870	8000.120163	10.797491	-0.058756	4.816009
285.863343	8000.166963	10.802496	-0.058775	4.816022
285.964312	8000.135695	10.807501	-0.058794	4.816012
285.840668	8000.078949	10.812506	-0.058771	4.815996
285.771078	8000.147172	10.817511	-0.058758	4.816017
285.663313	8000.164465	10.822515	-0.058739	4.816022
285.747217	8000.188463	10.827520	-0.058754	4.816029
285.914426	8000.169092	10.832525	-0.058786	4.816022
285.791085	8000.123039	10.837530	-0.058763	4.816010
285.818816	8000.170595	10.842535	-0.058768	4.816023
285.934945	8000.134259	10.847539	-0.058790	4.816012
285.721615	8000.132523	10.852544	-0.058751	4.816013
285.865019	8000.095616	10.857549	-0.058778	4.816001
285.807397	8000.090310	10.862554	-0.058767	4.816000
285.883877	8000.154787	10.867559	-0.058782	4.816018
285.614433	8000.159508	10.872563	-0.058732	4.816021
285.646961	8000.191119	10.877568	-0.058738	4.816030
285.757361	8000.182467	10.882573	-0.058759	4.816027
285.382360	8000.128615	10.887578	-0.058689	4.816013
285.729529	8000.183070	10.892583	-0.058754	4.816027
285.734121	8000.142560	10.897587	-0.058755	4.816015
285.590709	8000.082248	10.902592	-0.058729	4.815999
285.589470	8000.150650	10.907597	-0.058729	4.816019
285.720532	8000.069696	10.912602	-0.058753	4.815994
285.813294	8000.100269	10.917607	-0.058771	4.816003
285.681712	8000.050860	10.922611	-0.058746	4.815989
285.883397	8000.129380	10.927616	-0.058784	4.816011
285.799912	8000.155666	10.932621	-0.058769	4.816019
285.677450	8000.112837	10.937626	-0.058746	4.816007
285.816011	8000.186998	10.942631	-0.058772	4.816028
285.716632	8000.113594	10.947635	-0.058754	4.816007
285.738334	8000.072328	10.952640	-0.058758	4.815995
286.010154	8000.112582	10.957645	-0.058809	4.816005
286.038720	8000.108850	10.962650	-0.058815	4.816004
285.803148	8000.144116	10.967655	-0.058771	4.816015
285.767244	8000.154170	10.972659	-0.058764	4.816019
285.870167	8000.133625	10.977664	-0.058784	4.816012
286.036250	8000.166605	10.982669	-0.058815	4.816021
285.786251	8000.079763	10.987674	-0.058769	4.815997
285.803863	8000.181643	10.992679	-0.058772	4.816026
285.845508	8000.146085	10.997683	-0.058780	4.816016
285.879174	8000.167028	11.002688	-0.058787	4.816022
285.981794	8000.120826	11.007693	-0.058806	4.816008
286.052457	8000.095417	11.012698	-0.058819	4.816000
286.083182	8000.185780	11.017703	-0.058825	4.816026
285.871614	8000.099639	11.022707	-0.058786	4.816002
285.971581	8000.137825	11.027712	-0.058805	4.816013
285.901961	8000.147263	11.032717	-0.058792	4.816016
285.852809	8000.132493	11.037722	-0.058783	4.816012
285.831994	8000.187712	11.042727	-0.058780	4.816028
286.040118	8000.095339	11.047731	-0.058818	4.816000
285.803308	8000.132721	11.052736	-0.058775	4.816012
285.857292	8000.127315	11.057741	-0.058785	4.816010
285.687631	8000.111413	11.062746	-0.058753	4.816006
285.909606	8000.133656	11.067751	-0.058795	4.816012
285.904397	8000.079073	11.072755	-0.058794	4.815996
285.890857	8000.046782	11.077760	-0.058792	4.815986
285.924980	8000.161790	11.082765	-0.058799	4.816020
285.855611	8000.084658	11.087770	-0.058786	4.815998
285.925777	8000.149020	11.092775	-0.058799	4.816016
285.967242	8000.134835	11.097779	-0.058807	4.816012
286.045065	8000.152310	11.102784	-0.058822	4.816016
285.963410	8000.149771	11.107789	-0.058807	4.816016
285.928561	8000.097852	11.112794	-0.058800	4.816001
285.959046	8000.159353	11.117799	-0.058806	4.816019
285.952927	8000.125060	11.122803	-0.058805	4.816009
285.823909	8000.061803	11.127808	-0.058782	4.815991
286.069566	8000.084479	11.132813	-0.058828	4.815996
285.962597	8000.068653	11.137818	-0.058808	4.815992
285.983652	8000.204798	11.142823	-0.058812	4.816032
286.038467	8000.141691	11.147827	-0.058822	4.816013
286.127513	8000.148682	11.152832	-0.058839	4.816015
285.977885	8000.157728	11.157837	-0.058812	4.816018
286.084123	8000.110523	11.162842	-0.058832	4.816004
286.161860	8000.137616	11.167847	-0.058846	4.816011
286.059611	8000.173178	11.172851	-0.058828	4.816022
286.070310	8000.116747	11.177856	-0.058830	4.816006
286.173053	8000.177430	11.182861	-0.058849	4.816023
285.994093	8000.131430	11.187866	-0.058816	4.816010
286.086574	8000.197270	11.192871	-0.058833	4.816029
285.991993	8000.130365	11.197875	-0.058816	4.816010
286.048473	8000.130349	11.202880	-0.058827	4.816010
286.093221	8000.196385	11.207885	-0.058835	4.816029
286.058424	8000.129504	11.212890	-0.058829	4.816010
286.254936	8000.166247	11.217895	-0.058866	4.816019
285.869097	8000.132502	11.222899	-0.058794	4.816011
285.936212	8000.117717	11.227904	-0.058807	4.816007
285.994814	8000.155148	11.232909	-0.058818	4.816017
285.811572	8000.089832	11.237914	-0.058784	4.815999
286.022190	8000.153552	11.242919	-0.058824	4.816017
286.046126	8000.117670	11.247923	-0.058828	4.816006
286.035688	8000.149565	11.252928	-0.058826	4.816015
286.211513	8000.168830	11.257933	-0.058859	4.816020
286.035733	8000.134645	11.262938	-0.058827	4.816011
286.223762	8000.185128	11.267943	-0.058862	4.816025
286.295944	8000.129819	11.272947	-0.058876	4.816008
286.239532	8000.138430	11.277952	-0.058866	4.816011
286.192052	8000.177130	11.282957	-0.058857	4.816023
286.150145	8000.090880	11.287962	-0.058849	4.815998
286.139827	8000.140948	11.292967	-0.058848	4.816012
286.081558	8000.111047	11.297971	-0.058837	4.816004
286.179941	8000.115002	11.302976	-0.058855	4.816005
286.136335	8000.154842	11.307981	-0.058848	4.816016
286.020785	8000.113207	11.312986	-0.058826	4.816005
286.161622	8000.121143	11.317991	-0.058853	4.816006
286.052813	8000.137348	11.322995	-0.058833	4.816012
286.023468	8000.091943	11.328000	-0.058827	4.815999
286.135410	8000.151724	11.333005	-0.058848	4.816015
286.225658	8000.152324	11.338010	-0.058866	4.816015
286.273717	8000.147879	11.343015	-0.058875	4.816014
285.970689	8000.166950	11.348019	-0.058818	4.816021
286.038561	8000.160728	11.353024	-0.058831	4.816019
286.106706	8000.158787	11.358029	-0.058844	4.816018
286.123940	8000.129196	11.363034	-0.058848	4.816009
286.253463	8000.173267	11.368039	-0.058872	4.816021
286.051790	8000.096925	11.373043	-0.058835	4.816000
286.092279	8000.099823	11.378048	-0.058842	4.816000
286.402234	8000.135431	11.383053	-0.058900	4.816009
286.319235	8000.052706	11.388058	-0.058885	4.815985
286.266655	8000.149030	11.393063	-0.058876	4.816014
285.967908	8000.150009	11.398067	-0.058820	4.816016
286.225601	8000.087399	11.403072	-0.058868	4.815996
286.286815	8000.104571	11.408077	-0.058880	4.816001
286.240391	8000.081299	11.413082	-0.058871	4.815994
286.104254	8000.105555	11.418087	-0.058846	4.816002
286.121690	8000.100550	11.423091	-0.058850	4.816000
286.145035	8000.098860	11.428096	-0.058854	4.816000
286.128957	8000.140272	11.433101	-0.058852	4.816012
286.021876	8000.066726	11.438106	-0.058832	4.815991
285.975014	8000.108645	11.443111	-0.058823	4.816004
285.987652	8000.097140	11.448115	-0.058826	4.816000
286.100867	8000.107778	11.453120	-0.058847	4.816003
286.160505	8000.118508	11.458125	-0.058859	4.816005
286.060280	8000.099598	11.463130	-0.058840	4.816000
286.081735	8000.069015	11.468135	-0.058844	4.815991
286.225821	8000.121902	11.473139	-0.058871	4.816006
286.184516	8000.088035	11.478144	-0.058864	4.815996
286.371590	8000.134225	11.483149	-0.058899	4.816009
286.247111	8000.068912	11.488154	-0.058876	4.815990
286.161317	8000.103707	11.493159	-0.058860	4.816001
286.105873	8000.074926	11.498163	-0.058850	4.815993
286.252668	8000.162065	11.503168	-0.058878	4.816018
286.470883	8000.166071	11.508173	-0.058919	4.816018
286.261440	8000.086381	11.513178	-0.058880	4.815995
286.519926	8000.178767	11.518183	-0.058928	4.816021
286.250269	8000.162106	11.523187	-0.058878	4.816018
286.183984	8000.124576	11.528192	-0.058866	4.816007
286.207011	8000.161358	11.533197	-0.058870	4.816018
286.223282	8000.114648	11.538202	-0.058874	4.816004
286.438387	8000.153869	11.543207	-0.058914	4.816014
286.176300	8000.107419	11.548211	-0.058865	4.816002
286.214476	8000.127376	11.553216	-0.058873	4.816008
286.539517	8000.179293	11.558221	-0.058933	4.816021
286.168224	8000.098785	11.563226	-0.058864	4.816000
286.224045	8000.107307	11.568231	-0.058875	4.816002
286.364785	8000.143032	11.573235	-0.058902	4.816011
286.287587	8000.124542	11.578240	-0.058887	4.816006
286.316688	8000.162503	11.583245	-0.058893	4.816017
286.246133	8000.072523	11.588250	-0.058880	4.815991
286.393631	8000.138299	11.593255	-0.058908	4.816010
286.494548	8000.159402	11.598259	-0.058927	4.816015
286.511493	8000.092396	11.603264	-0.058930	4.815996
286.550493	8000.183980	11.608269	-0.058938	4.816022
286.405708	8000.149292	11.613274	-0.058911	4.816013
286.642420	8000.167531	11.618279	-0.058955	4.816017
286.420033	8000.148527	11.623283	-0.058914	4.816013
286.419438	8000.130367	11.628288	-0.058914	4.816007
286.344145	8000.188868	11.633293	-0.058900	4.816025
286.335002	8000.195135	11.638298	-0.058899	4.816027
286.409670	8000.208277	11.643303	-0.058913	4.816030
286.500371	8000.214230	11.648307	-0.058930	4.816031
286.437761	8000.174630	11.653312	-0.058919	4.816020
286.356828	8000.190274	11.658317	-0.058904	4.816025
286.136630	8000.129626	11.663322	-0.058863	4.816009
286.233471	8000.169893	11.668327	-0.058881	4.816020
286.305808	8000.138102	11.673331	-0.058895	4.816010
286.269544	8000.101120	11.678336	-0.058888	4.816000
286.209617	8000.155626	11.683341	-0.058877	4.816016
286.244417	8000.099635	11.688346	-0.058884	4.815999
286.518947	8000.129253	11.693351	-0.058935	4.816006
286.400968	8000.137807	11.698355	-0.058914	4.816010
286.600624	8000.144681	11.703360	-0.058951	4.816010
286.518565	8000.190233	11.708365	-0.058936	4.816024
286.463316	8000.135803	11.713370	-0.058926	4.816009
286.598607	8000.186393	11.718375	-0.058951	4.816023
286.590471	8000.152062	11.723379	-0.058950	4.816013
286.344271	8000.132623	11.728384	-0.058904	4.816008
286.457437	8000.149675	11.733389	-0.058926	4.816013
286.393393	8000.085465	11.738394	-0.058914	4.815994
286.401889	8000.172217	11.743399	-0.058916	4.816020
286.374659	8000.166397	11.748403	-0.058911	4.816018
286.249184	8000.175884	11.753408	-0.058888	4.816021
286.371066	8000.142859	11.758413	-0.058911	4.816011
286.266721	8000.081120	11.763418	-0.058891	4.815994
286.304766	8000.160929	11.768423	-0.058899	4.816017
286.533684	8000.175820	11.773427	-0.058942	4.816020
286.286952	8000.128581	11.778432	-0.058896	4.816007
286.393632	8000.179717	11.783437	-0.058916	4.816022
286.223234	8000.119978	11.788442	-0.058884	4.816005
286.343241	8000.188459	11.793447	-0.058907	4.816025
286.566279	8000.198966	11.798451	-0.058949	4.816026
286.371024	8000.190077	11.803456	-0.058913	4.816025
286.570639	8000.231154	11.808461	-0.058950	4.816036
286.586480	8000.150232	11.813466	-0.058953	4.816012
286.482386	8000.159040	11.818471	-0.058934	4.816015
286.429768	8000.183753	11.823475	-0.058924	4.816023
286.641389	8000.222911	11.828480	-0.058964	4.816033
286.700492	8000.244320	11.833485	-0.058975	4.816039
286.621655	8000.147774	11.838490	-0.058961	4.816011
286.673909	8000.142336	11.843495	-0.058971	4.816009
286.488456	8000.162484	11.848499	-0.058936	4.816016
286.412717	8000.161122	11.853504	-0.058923	4.816016
286.480993	8000.159184	11.858509	-0.058935	4.816015
286.577244	8000.143861	11.863514	-0.058954	4.816010
286.719054	8000.173194	11.868519	-0.058980	4.816018
286.590813	8000.164460	11.873523	-0.058957	4.816016
286.659886	8000.144365	11.878528	-0.058970	4.816010
286.825745	8000.189101	11.883533	-0.059001	4.816022
286.382164	8000.110477	11.888538	-0.058918	4.816001
286.706924	8000.182697	11.893543	-0.058979	4.816021
286.553850	8000.188473	11.898547	-0.058951	4.816023
286.328745	8000.159800	11.903552	-0.058909	4.816016
286.514132	8000.216649	11.908557	-0.058944	4.816032
286.606755	8000.204467	11.913562	-0.058961	4.816028
286.543449	8000.199056	11.918567	-0.058950	4.816026
286.554358	8000.209965	11.923571	-0.058952	4.816030
286.539703	8000.137037	11.928576	-0.058949	4.816008
286.624674	8000.185639	11.933581	-0.058965	4.816022
286.413165	8000.164696	11.938586	-0.058926	4.816017
286.598144	8000.165958	11.943591	-0.058961	4.816016
286.567883	8000.187872	11.948595	-0.058956	4.816023
286.624464	8000.158999	11.953600	-0.058966	4.816014
286.451932	8000.162282	11.958605	-0.058934	4.816016
286.532191	8000.157356	11.963610	-0.058950	4.816014
286.745301	8000.175165	11.968615	-0.058989	4.816018
286.498405	8000.159988	11.973619	-0.058944	4.816015
286.562628	8000.170801	11.978624	-0.058956	4.816018
286.569652	8000.183777	11.983629	-0.058957	4.816022
286.409119	8000.127424	11.988634	-0.058928	4.816006
286.656303	8000.185402	11.993639	-0.058974	4.816022
286.742576	8000.191274	11.998643	-0.058990	4.816023
286.732060	8000.118422	12.003648	-0.058988	4.816002
286.666696	8000.177104	12.008653	-0.058977	4.816019
286.690759	8000.119847	12.013658	-0.058981	4.816002
286.688697	8000.146552	12.018663	-0.058981	4.816010
286.606743	8000.154696	12.023667	-0.058966	4.816013
286.471942	8000.134085	12.028672	-0.058941	4.816008
286.722498	8000.209226	12.033677	-0.058988	4.816028
286.603894	8000.149363	12.038682	-0.058966	4.816011
286.683296	8000.149765	12.043687	-0.058981	4.816011
286.571841	8000.180885	12.048691	-0.058961	4.816021
286.320465	8000.158145	12.053696	-0.058914	4.816015
286.438021	8000.238338	12.058701	-0.058936	4.816038
286.547773	8000.197610	12.063706	-0.058957	4.816026
286.785590	8000.184874	12.068711	-0.059001	4.816021
286.742938	8000.191598	12.073715	-0.058994	4.816023
286.753432	8000.208912	12.078720	-0.058996	4.816028
286.664217	8000.217992	12.083725	-0.058979	4.816031
286.513309	8000.166090	12.088730	-0.058951	4.816017
286.707251	8000.181411	12.093735	-0.058988	4.816020
286.773596	8000.147372	12.098739	-0.059000	4.816010
286.784886	8000.116603	12.103744	-0.059003	4.816001
286.616101	8000.149882	12.108749	-0.058971	4.816011
286.617287	8000.131754	12.113754	-0.058972	4.816006
286.691626	8000.119238	12.118759	-0.058986	4.816002
286.485750	8000.128325	12.123763	-0.058948	4.816006
286.445654	8000.078447	12.128768	-0.058940	4.815991
286.455257	8000.170564	12.133773	-0.058943	4.816018
286.302478	8000.106871	12.138778	-0.058914	4.816000
286.480720	8000.153970	12.143783	-0.058948	4.816013
286.659520	8000.176496	12.148787	-0.058981	4.816019
286.719690	8000.192580	12.153792	-0.058993	4.816023
286.661189	8000.251388	12.158797	-0.058982	4.816041
286.622653	8000.204745	12.163802	-0.058975	4.816027
286.761327	8000.216919	12.168807	-0.059001	4.816030
286.651440	8000.219208	12.173811	-0.058981	4.816031
286.671611	8000.196083	12.178816	-0.058985	4.816025
286.667172	8000.205642	12.183821	-0.058984	4.816027
286.439108	8000.184396	12.188826	-0.058942	4.816022
286.462052	8000.154909	12.193831	-0.058946	4.816014
286.492104	8000.130896	12.198835	-0.058952	4.816006
286.608641	8000.195038	12.203840	-0.058974	4.816025
286.434957	8000.168372	12.208845	-0.058942	4.816018
286.505722	8000.144034	12.213850	-0.058955	4.816010
286.575847	8000.167781	12.218855	-0.058969	4.816017
286.633030	8000.176329	12.223859	-0.058979	4.816019
286.787931	8000.155665	12.228864	-0.059009	4.816012
286.688616	8000.168836	12.233869	-0.058990	4.816016
286.515134	8000.076974	12.238874	-0.058958	4.815990
286.634744	8000.131553	12.243879	-0.058981	4.816006
286.804098	8000.173146	12.248883	-0.059012	4.816017
286.765892	8000.129715	12.253888	-0.059005	4.816005
286.709980	8000.197122	12.258893	-0.058995	4.816025
286.708738	8000.139402	12.263898	-0.058995	4.816008
286.796362	8000.155988	12.268903	-0.059012	4.816012
286.439466	8000.183693	12.273907	-0.058946	4.816022
286.611660	8000.154794	12.278912	-0.058978	4.816013
286.759963	8000.200278	12.283917	-0.059006	4.816025
286.820478	8000.177890	12.288922	-0.059017	4.816018
286.832595	8000.157824	12.293927	-0.059020	4.816012
286.706601	8000.203642	12.298931	-0.058996	4.816026
286.618430	8000.168918	12.303936	-0.058980	4.816017
286.790145	8000.224450	12.308941	-0.059012	4.816032
286.673873	8000.179593	12.313946	-0.058991	4.816020
286.551711	8000.178451	12.318951	-0.058968	4.816020
286.574584	8000.191716	12.323955	-0.058973	4.816024
286.423822	8000.180433	12.328960	-0.058945	4.816021
286.331995	8000.172364	12.333965	-0.058928	4.816019
286.308590	8000.174095	12.338970	-0.058924	4.816020
286.265175	8000.174392	12.343975	-0.058916	4.816020
286.627449	8000.194925	12.348979	-0.058984	4.816024
286.367911	8000.161347	12.353984	-0.058936	4.816016
286.438013	8000.206471	12.358989	-0.058949	4.816029
286.328024	8000.170281	12.363994	-0.058929	4.816019
286.578034	8000.199451	12.368999	-0.058976	4.816026
286.651104	8000.212565	12.374003	-0.058989	4.816029
286.446736	8000.150066	12.379008	-0.058951	4.816012
286.467125	8000.207109	12.384013	-0.058956	4.816029
286.363187	8000.163547	12.389018	-0.058936	4.816016
286.292628	8000.119526	12.394023	-0.058923	4.816004
286.559947	8000.196041	12.399027	-0.058973	4.816025
286.611939	8000.138226	12.404032	-0.058983	4.816008
286.632043	8000.164266	12.409037	-0.058987	4.816015
286.510835	8000.144972	12.414042	-0.058965	4.816010
286.803306	8000.183470	12.419047	-0.059020	4.816020
286.766686	8000.195648	12.424051	-0.059013	4.816024
286.650014	8000.122994	12.429056	-0.058991	4.816003
286.776585	8000.209766	12.434061	-0.059015	4.816028
286.569650	8000.117293	12.439066	-0.058977	4.816002
286.625475	8000.094819	12.444071	-0.058988	4.815995
286.589990	8000.172218	12.449075	-0.058981	4.816018
286.651746	8000.154128	12.454080	-0.058993	4.816012
286.688384	8000.156956	12.459085	-0.059000	4.816013
286.632851	8000.138861	12.464090	-0.058990	4.816008
286.775638	8000.113700	12.469095	-0.059017	4.816000
286.663647	8000.185426	12.474099	-0.058996	4.816021
286.700670	8000.145507	12.479104	-0.059003	4.816009
286.770566	8000.114740	12.484109	-0.059016	4.816000
286.860735	8000.100375	12.489114	-0.059033	4.815995
286.754627	8000.123042	12.494119	-0.059014	4.816002
286.799809	8000.132439	12.499123	-0.059022	4.816005
286.851379	8000.120576	12.504128	-0.059032	4.816001
286.725964	8000.172817	12.509133	-0.059009	4.816017
286.588694	8000.079479	12.514138	-0.058984	4.815990
286.826660	8000.098811	12.519143	-0.059028	4.815995
286.753396	8000.146661	12.524147	-0.059015	4.816009
286.598450	8000.140645	12.529152	-0.058986	4.816008
286.954814	8000.195274	12.534157	-0.059053	4.816022
286.816234	8000.139321	12.539162	-0.059027	4.816007
286.587530	8000.136234	12.544167	-0.058985	4.816007
286.727195	8000.179422	12.549171	-0.059011	4.816019
286.702667	8000.127690	12.554176	-0.059007	4.816004
286.820433	8000.215371	12.559181	-0.059029	4.816029
286.687193	8000.190512	12.564186	-0.059004	4.816022
286.762916	8000.186572	12.569191	-0.059019	4.816021
286.915683	8000.169076	12.574195	-0.059047	4.816015
286.803453	8000.144601	12.579200	-0.059026	4.816008
286.858938	8000.211904	12.584205	-0.059037	4.816028
286.840581	8000.170974	12.589210	-0.059034	4.816016
286.886313	8000.165417	12.594215	-0.059043	4.816014
286.895096	8000.192320	12.599219	-0.059044	4.816022
286.816177	8000.119286	12.604224	-0.059030	4.816001
287.005451	8000.128109	12.609229	-0.059065	4.816002
286.880003	8000.189970	12.614234	-0.059042	4.816021
286.916050	8000.167135	12.619239	-0.059049	4.816014
286.855228	8000.147874	12.624243	-0.059038	4.816009
286.664494	8000.119828	12.629248	-0.059003	4.816002
286.812850	8000.247615	12.634253	-0.059031	4.816038
286.786705	8000.193716	12.639258	-0.059026	4.816023
286.720098	8000.195726	12.644263	-0.059014	4.816024
286.774187	8000.152913	12.649267	-0.059024	4.816011
286.828728	8000.190271	12.654272	-0.059034	4.816021
286.847040	8000.234450	12.659277	-0.059038	4.816034
286.776215	8000.176528	12.664282	-0.059025	4.816018
286.837714	8000.239666	12.669287	-0.059037	4.816036
287.102487	8000.227423	12.674291	-0.059086	4.816031
286.869613	8000.143025	12.679296	-0.059043	4.816007
286.794496	8000.196186	12.684301	-0.059029	4.816023
286.855890	8000.177020	12.689306	-0.059041	4.816017
286.938245	8000.179615	12.694311	-0.059057	4.816018
286.904601	8000.210018	12.699315	-0.059051	4.816027
287.179897	8000.177659	12.704320	-0.059102	4.816016
287.018380	8000.207863	12.709325	-0.059072	4.816025
286.943416	8000.179794	12.714330	-0.059058	4.816018
287.096416	8000.200781	12.719335	-0.059087	4.816023
287.082502	8000.245440	12.724339	-0.059085	4.816036
286.999413	8000.150952	12.729344	-0.059069	4.816009
287.146246	8000.212443	12.734349	-0.059097	4.816026
286.897733	8000.202580	12.739354	-0.059051	4.816025
286.989822	8000.238487	12.744359	-0.059068	4.816035
286.802156	8000.254319	12.749363	-0.059034	4.816040
286.838393	8000.206903	12.754368	-0.059041	4.816026
286.917223	8000.243637	12.759373	-0.059055	4.816036
286.683848	8000.205191	12.764378	-0.059012	4.816026
286.842364	8000.199557	12.769383	-0.059042	4.816024
286.984151	8000.205375	12.774387	-0.059069	4.816025
286.896651	8000.143942	12.779392	-0.059052	4.816007
286.760069	8000.205599	12.784397	-0.059027	4.816026
286.827825	8000.202582	12.789402	-0.059040	4.816025
286.945638	8000.209031	12.794407	-0.059062	4.816026
287.004779	8000.174861	12.799411	-0.059073	4.816016
286.945616	8000.146011	12.804416	-0.059063	4.816008
286.901586	8000.171949	12.809421	-0.059055	4.816015
286.785943	8000.186959	12.814426	-0.059033	4.816020
286.920467	8000.127444	12.819431	-0.059059	4.816002
287.186071	8000.237066	12.824435	-0.059108	4.816033
287.080921	8000.143244	12.829440	-0.059089	4.816006
286.977564	8000.195889	12.834445	-0.059070	4.816022
286.988357	8000.187556	12.839450	-0.059072	4.816020
287.023442	8000.147601	12.844455	-0.059079	4.816008
286.954642	8000.214773	12.849459	-0.059066	4.816028
286.809913	8000.156569	12.854464	-0.059040	4.816011
287.063612	8000.246734	12.859469	-0.059087	4.816036
286.970461	8000.212987	12.864474	-0.059070	4.816027
286.918149	8000.202433	12.869479	-0.059060	4.816024
287.088536	8000.210911	12.874483	-0.059092	4.816026
286.870703	8000.155648	12.879488	-0.059052	4.816011
287.004830	8000.186978	12.884493	-0.059077	4.816019
286.978809	8000.157665	12.889498	-0.059073	4.816011
287.141356	8000.183102	12.894503	-0.059103	4.816017
287.211368	8000.194022	12.899507	-0.059116	4.816020
286.917097	8000.151256	12.904512	-0.059062	4.816009
287.083551	8000.228070	12.909517	-0.059093	4.816031
286.828927	8000.182823	12.914522	-0.059046	4.816019
286.928324	8000.166489	12.919527	-0.059064	4.816014
287.077316	8000.224813	12.924531	-0.059092	4.816030
287.007906	8000.129506	12.929536	-0.059080	4.816002
286.932583	8000.159148	12.934541	-0.059066	4.816011
286.905365	8000.157603	12.939546	-0.059061	4.816011
287.063087	8000.101719	12.944551	-0.059091	4.815994
287.009601	8000.194822	12.949555	-0.059081	4.816021
286.709769	8000.109202	12.954560	-0.059025	4.815998
286.950808	8000.156380	12.959565	-0.059070	4.816010
287.145786	8000.167445	12.964570	-0.059107	4.816013
286.887846	8000.163823	12.969575	-0.059059	4.816013
287.078659	8000.212222	12.974579	-0.059095	4.816026
287.019765	8000.173757	12.979584	-0.059084	4.816015
287.137403	8000.245404	12.984589	-0.059106	4.816035
286.997614	8000.197979	12.989594	-0.059080	4.816022
287.035202	8000.183722	12.994599	-0.059088	4.816018
287.173090	8000.233293	12.999603	-0.059113	4.816032
286.799671	8000.153809	13.004608	-0.059044	4.816010
287.008601	8000.160854	13.009613	-0.059083	4.816011
286.832608	8000.150178	13.014618	-0.059051	4.816009
286.892493	8000.210080	13.019623	-0.059062	4.816026
286.878658	8000.232295	13.024627	-0.059060	4.816033
286.978179	8000.135799	13.029632	-0.059078	4.816004
286.940298	8000.208879	13.034637	-0.059072	4.816026
286.985985	8000.208666	13.039642	-0.059080	4.816025
286.856952	8000.157162	13.044647	-0.059056	4.816011
287.133996	8000.216757	13.049651	-0.059108	4.816027
286.886707	8000.149197	13.054656	-0.059062	4.816009
286.973661	8000.177529	13.059661	-0.059079	4.816016
287.056862	8000.170519	13.064666	-0.059095	4.816014
286.785760	8000.169863	13.069671	-0.059044	4.816015
286.892137	8000.202824	13.074675	-0.059064	4.816024
286.921503	8000.127493	13.079680	-0.059070	4.816002
286.905067	8000.144315	13.084685	-0.059067	4.816007
286.822596	8000.135348	13.089690	-0.059052	4.816005
287.115216	8000.086203	13.094695	-0.059107	4.815989
287.264144	8000.147732	13.099699	-0.059135	4.816006
287.105677	8000.070038	13.104704	-0.059105	4.815984
287.111915	8000.142856	13.109709	-0.059107	4.816005
287.047408	8000.098944	13.114714	-0.059095	4.815993
286.905807	8000.082483	13.119719	-0.059069	4.815989
286.916776	8000.121183	13.124723	-0.059071	4.816000
286.968155	8000.096491	13.129728	-0.059081	4.815993
287.088888	8000.114750	13.134733	-0.059104	4.815997
287.021327	8000.097504	13.139738	-0.059091	4.815993
287.109449	8000.144027	13.144743	-0.059108	4.816006
287.165491	8000.186758	13.149747	-0.059118	4.816018
287.042224	8000.096880	13.154752	-0.059096	4.815992
287.225421	8000.172931	13.159757	-0.059130	4.816014
287.285621	8000.187947	13.164762	-0.059141	4.816018
287.089490	8000.159801	13.169767	-0.059105	4.816010
287.165292	8000.215719	13.174771	-0.059120	4.816026
286.991574	8000.138815	13.179776	-0.059087	4.816005
287.042617	8000.195349	13.184781	-0.059097	4.816021
287.135394	8000.184239	13.189786	-0.059115	4.816017
286.828496	8000.208582	13.194791	-0.059058	4.816026
287.136300	8000.230259	13.199795	-0.059115	4.816031
287.123104	8000.152012	13.204800	-0.059113	4.816008
287.104485	8000.185897	13.209805	-0.059110	4.816018
287.063461	8000.161653	13.214810	-0.059102	4.816011
287.120877	8000.126382	13.219815	-0.059113	4.816000
287.031760	8000.189976	13.224819	-0.059097	4.816020
287.199751	8000.119315	13.229824	-0.059128	4.815998
287.168349	8000.190376	13.234829	-0.059123	4.816019
287.027212	8000.213471	13.239834	-0.059097	4.816026
286.990166	8000.093103	13.244839	-0.059090	4.815991
287.076073	8000.166307	13.249843	-0.059106	4.816012
286.986304	8000.131554	13.254848	-0.059090	4.816003
286.923601	8000.208456	13.259853	-0.059078	4.816025
286.954700	8000.191944	13.264858	-0.059084	4.816020
287.048450	8000.194746	13.269863	-0.059102	4.816021
286.934049	8000.199091	13.274867	-0.059081	4.816023
287.095825	8000.152900	13.279872	-0.059111	4.816008
287.258285	8000.195437	13.284877	-0.059142	4.816020
287.140684	8000.185827	13.289882	-0.059120	4.816018
287.198070	8000.099250	13.294887	-0.059131	4.815992
287.222171	8000.158499	13.299891	-0.059135	4.816009
287.098077	8000.155184	13.304896	-0.059113	4.816009
287.167363	8000.148989	13.309901	-0.059126	4.816007
287.354801	8000.196259	13.314906	-0.059161	4.816020
287.297609	8000.142860	13.319911	-0.059150	4.816004
287.046335	8000.181045	13.324915	-0.059104	4.816017
287.103511	8000.072018	13.329920	-0.059115	4.815985
287.302650	8000.136602	13.334925	-0.059152	4.816002
287.173021	8000.112878	13.339930	-0.059128	4.815996
287.217851	8000.140440	13.344935	-0.059137	4.816004
287.191471	8000.221213	13.349939	-0.059132	4.816028
287.095764	8000.146802	13.354944	-0.059114	4.816006
286.877519	8000.179177	13.359949	-0.059074	4.816017
286.962411	8000.108067	13.364954	-0.059090	4.815996
287.055099	8000.130090	13.369959	-0.059107	4.816002
286.907454	8000.178719	13.374963	-0.059080	4.816017
287.131136	8000.087698	13.379968	-0.059122	4.815989
287.251761	8000.174363	13.384973	-0.059145	4.816014
286.940346	8000.164419	13.389978	-0.059087	4.816012
286.977496	8000.170463	13.394983	-0.059094	4.816014
287.274346	8000.193010	13.399987	-0.059150	4.816019
287.157707	8000.185556	13.404992	-0.059128	4.816017
287.233172	8000.188024	13.409997	-0.059142	4.816018
287.284338	8000.194325	13.415002	-0.059152	4.816019
287.250566	8000.126390	13.420007	-0.059146	4.816000
287.139137	8000.194921	13.425011	-0.059125	4.816020
287.229137	8000.123903	13.430016	-0.059142	4.815999
287.374031	8000.185360	13.435021	-0.059170	4.816016
287.186437	8000.173402	13.440026	-0.059135	4.816014
287.232954	8000.152896	13.445031	-0.059144	4.816007
287.389524	8000.179293	13.450035	-0.059173	4.816014
286.940510	8000.111254	13.455040	-0.059090	4.815997
287.073581	8000.197077	13.460045	-0.059115	4.816021
287.311394	8000.155482	13.465050	-0.059159	4.816008
287.227041	8000.167858	13.470055	-0.059144	4.816012
287.291567	8000.204330	13.475059	-0.059156	4.816022
287.313007	8000.133129	13.480064	-0.059160	4.816001
287.237823	8000.198046	13.485069	-0.059146	4.816020
287.131969	8000.162998	13.490074	-0.059127	4.816011
287.091252	8000.133416	13.495079	-0.059119	4.816002
287.250490	8000.190859	13.500083	-0.059149	4.816018
287.151965	8000.113190	13.505088	-0.059131	4.815996
287.084190	8000.149384	13.510093	-0.059119	4.816007
287.019204	8000.159975	13.515098	-0.059107	4.816010
287.097539	8000.113328	13.520103	-0.059122	4.815996
287.150101	8000.192337	13.525107	-0.059132	4.816019
287.075567	8000.176032	13.530112	-0.059118	4.816015
287.109660	8000.217293	13.535117	-0.059125	4.816027
287.033110	8000.193469	13.540122	-0.059111	4.816020
286.995847	8000.112645	13.545127	-0.059104	4.815997
287.231100	8000.158650	13.550131	-0.059148	4.816009
287.129090	8000.125810	13.555136	-0.059129	4.816000
287.313073	8000.164466	13.560141	-0.059164	4.816010
287.266791	8000.190363	13.565146	-0.059155	4.816018
287.273022	8000.078267	13.570151	-0.059157	4.815985
287.304851	8000.175067	13.575155	-0.059163	4.816013
287.178542	8000.183469	13.580160	-0.059139	4.816016
287.336635	8000.186379	13.585165	-0.059169	4.816016
287.388269	8000.193757	13.590170	-0.059179	4.816018
287.170361	8000.167350	13.595175	-0.059139	4.816012
287.310064	8000.244745	13.600179	-0.059165	4.816034
287.341878	8000.173733	13.605184	-0.059171	4.816013
287.083190	8000.226746	13.610189	-0.059123	4.816030
287.081827	8000.180781	13.615194	-0.059123	4.816016
287.224363	8000.204784	13.620199	-0.059150	4.816022
287.247427	8000.245844	13.625203	-0.059154	4.816034
287.030732	8000.120055	13.630208	-0.059114	4.815999
287.100397	8000.148070	13.635213	-0.059127	4.816006
287.166745	8000.172819	13.640218	-0.059140	4.816013
287.106916	8000.139681	13.645223	-0.059129	4.816004
287.390446	8000.225048	13.650227	-0.059182	4.816027
287.375611	8000.128599	13.655232	-0.059179	4.815999
287.274147	8000.141731	13.660237	-0.059161	4.816004
287.203731	8000.176807	13.665242	-0.059148	4.816014
287.103510	8000.194236	13.670247	-0.059129	4.816020
287.109647	8000.273466	13.675251	-0.059131	4.816043
287.178069	8000.192434	13.680256	-0.059144	4.816019
287.234774	8000.203111	13.685261	-0.059154	4.816022
287.284944	8000.224358	13.690266	-0.059164	4.816028
287.206773	8000.206917	13.695271	-0.059150	4.816023
287.268893	8000.257242	13.700275	-0.059161	4.816037
287.179749	8000.171193	13.705280	-0.059145	4.816013
287.064450	8000.200105	13.710285	-0.059124	4.816022
287.091717	8000.208106	13.715290	-0.059129	4.816024
287.162003	8000.200861	13.720295	-0.059142	4.816021
287.142688	8000.194116	13.725299	-0.059139	4.816020
287.077627	8000.188672	13.730304	-0.059127	4.816018
287.199445	8000.128925	13.735309	-0.059150	4.816000
287.107394	8000.207429	13.740314	-0.059133	4.816024
287.001660	8000.160626	13.745319	-0.059114	4.816010
287.239196	8000.220569	13.750323	-0.059158	4.816027
287.137635	8000.141776	13.755328	-0.059139	4.816004
287.177649	8000.168181	13.760333	-0.059147	4.816012
286.889149	8000.250577	13.765338	-0.059094	4.816037
287.184441	8000.223928	13.770343	-0.059149	4.816028
287.152324	8000.207329	13.775347	-0.059143	4.816023
287.184538	8000.216490	13.780352	-0.059149	4.816026
287.311880	8000.217769	13.785357	-0.059173	4.816025
287.140483	8000.203970	13.790362	-0.059141	4.816022
287.174628	8000.222786	13.795367	-0.059148	4.816028
287.156051	8000.244914	13.800371	-0.059145	4.816034
287.133997	8000.167573	13.805376	-0.059141	4.816012
287.179512	8000.164150	13.810381	-0.059150	4.816010
287.057585	8000.230351	13.815386	-0.059127	4.816030
287.069347	8000.207072	13.820391	-0.059129	4.816024
287.176226	8000.209046	13.825395	-0.059150	4.816024
287.290181	8000.142742	13.830400	-0.059171	4.816004
287.334992	8000.190612	13.835405	-0.059180	4.816017
287.103036	8000.173569	13.840410	-0.059137	4.816014
287.266436	8000.149854	13.845415	-0.059167	4.816006
287.378374	8000.233155	13.850419	-0.059188	4.816030
287.127399	8000.193317	13.855424	-0.059142	4.816019
287.210506	8000.183099	13.860429	-0.059157	4.816016
287.053198	8000.163144	13.865434	-0.059128	4.816011
287.272996	8000.134046	13.870439	-0.059169	4.816001
287.511127	8000.211102	13.875443	-0.059214	4.816022
287.324083	8000.199154	13.880448	-0.059179	4.816020
287.297546	8000.227550	13.885453	-0.059175	4.816028
287.465578	8000.219953	13.890458	-0.059206	4.816025
287.422099	8000.201009	13.895463	-0.059198	4.816020
287.200090	8000.208731	13.900467	-0.059157	4.816023
287.442630	8000.178980	13.905472	-0.059203	4.816013
287.362457	8000.247013	13.910477	-0.059188	4.816034
287.150657	8000.227130	13.915482	-0.059149	4.816029
287.071951	8000.167994	13.920487	-0.059134	4.816012
287.419446	8000.204294	13.925491	-0.059199	4.816021
287.050529	8000.178334	13.930496	-0.059131	4.816015
287.277396	8000.247702	13.935501	-0.059173	4.816034
287.548449	8000.222748	13.940506	-0.059224	4.816025
287.447513	8000.167480	13.945511	-0.059205	4.816010
287.366756	8000.207712	13.950515	-0.059190	4.816022
287.388511	8000.181409	13.955520	-0.059195	4.816014
287.475888	8000.216162	13.960525	-0.059211	4.816024
287.319411	8000.228288	13.965530	-0.059182	4.816028
287.252707	8000.213195	13.970535	-0.059170	4.816024
287.278077	8000.224368	13.975539	-0.059175	4.816027
287.094737	8000.201799	13.980544	-0.059141	4.816022
287.248755	8000.268767	13.985549	-0.059170	4.816040
287.354829	8000.238661	13.990554	-0.059190	4.816031
287.248639	8000.180091	13.995559	-0.059170	4.816015
287.121053	8000.231224	14.000563	-0.059147	4.816030
287.098090	8000.219068	14.005568	-0.059143	4.816027
287.313210	8000.246535	14.010573	-0.059183	4.816034
287.272743	8000.242610	14.015578	-0.059176	4.816033
287.122767	8000.223858	14.020583	-0.059148	4.816028
287.234548	8000.224853	14.025587	-0.059169	4.816028
287.261239	8000.195433	14.030592	-0.059174	4.816019
287.261149	8000.167662	14.035597	-0.059174	4.816011
287.251527	8000.183540	14.040602	-0.059173	4.816015
287.423250	8000.139669	14.045607	-0.059205	4.816002
287.489187	8000.222130	14.050611	-0.059218	4.816025
287.359008	8000.146019	14.055616	-0.059193	4.816004
287.572122	8000.162762	14.060621	-0.059233	4.816008
287.539462	8000.188908	14.065626	-0.059228	4.816015
287.259180	8000.176325	14.070631	-0.059176	4.816013
287.299721	8000.239082	14.075635	-0.059183	4.816031
287.172907	8000.144862	14.080640	-0.059160	4.816005
287.183367	8000.239135	14.085645	-0.059162	4.816032
287.391813	8000.241897	14.090650	-0.059201	4.816032
287.431086	8000.165676	14.095655	-0.059209	4.816009
287.509646	8000.204544	14.100659	-0.059223	4.816020
287.273767	8000.192772	14.105664	-0.059180	4.816018
287.129072	8000.169841	14.110669	-0.059153	4.816012
287.233492	8000.215594	14.115674	-0.059173	4.816025
287.004780	8000.207160	14.120679	-0.059130	4.816024
287.267727	8000.237639	14.125683	-0.059180	4.816031
287.124502	8000.221148	14.130688	-0.059153	4.816027
287.104432	8000.213320	14.135693	-0.059150	4.816025
287.228286	8000.163230	14.140698	-0.059173	4.816010
286.989230	8000.183467	14.145703	-0.059129	4.816017
287.380346	8000.204530	14.150707	-0.059202	4.816021
287.117107	8000.187983	14.155712	-0.059153	4.816017
287.175832	8000.242521	14.160717	-0.059164	4.816033
287.278336	8000.244416	14.165722	-0.059183	4.816033
287.129995	8000.215004	14.170727	-0.059156	4.816025
287.268029	8000.275267	14.175731	-0.059182	4.816042
287.228764	8000.212576	14.180736	-0.059175	4.816024
287.201179	8000.181095	14.185741	-0.059170	4.816015
287.180622	8000.199981	14.190746	-0.059166	4.816020
287.319588	8000.151235	14.195751	-0.059192	4.816005
287.364949	8000.229044	14.200755	-0.059201	4.816028
287.257520	8000.195036	14.205760	-0.059181	4.816019
287.323259	8000.229394	14.210765	-0.059194	4.816028
287.266558	8000.260445	14.215770	-0.059183	4.816038
287.114479	8000.191417	14.220775	-0.059155	4.816018
287.344699	8000.171061	14.225779	-0.059198	4.816011
287.208573	8000.199592	14.230784	-0.059173	4.816020
287.383586	8000.196398	14.235789	-0.059206	4.816018
287.422611	8000.213165	14.240794	-0.059213	4.816023
287.404464	8000.194684	14.245799	-0.059210	4.816018
287.391042	7999.222878	14.250803	-0.059207	4.815734

287.133317	7996.029183	14.255808	-0.059157	4.814802
287.165441	7990.607530	14.260813	-0.059160	4.813218
287.055046	7983.943193	14.265818	-0.059135	4.811270
287.100522	7976.615123	14.270823	-0.059139	4.809127
286.934806	7969.034835	14.275827	-0.059104	4.806910
286.977085	7961.198330	14.280832	-0.059107	4.804616
287.059723	7953.335342	14.285837	-0.059117	4.802313
286.870701	7945.377756	14.290842	-0.059077	4.799982
287.009971	7937.472203	14.295847	-0.059098	4.797664
286.895899	7929.403401	14.300851	-0.059072	4.795298
286.990823	7921.405875	14.305856	-0.059084	4.792951
286.902673	7913.341235	14.310861	-0.059063	4.790584
286.944687	7905.415537	14.315866	-0.059066	4.788256
286.656077	7897.370573	14.320871	-0.059007	4.785893
286.617557	7889.459929	14.325875	-0.058995	4.783568
286.576011	7881.410919	14.330880	-0.058982	4.781200
286.536885	7873.404138	14.335885	-0.058970	4.778844
286.305472	7865.462051	14.340890	-0.058922	4.776507
286.270907	7857.372168	14.345895	-0.058910	4.774124
286.407476	7849.385212	14.350899	-0.058931	4.771769
286.204885	7841.299893	14.355904	-0.058888	4.769386
286.267423	7833.401258	14.360909	-0.058895	4.767055
286.286644	7825.348307	14.365914	-0.058893	4.764678
286.055919	7817.434378	14.370919	-0.058845	4.762342
286.124666	7809.393290	14.375923	-0.058853	4.759966
285.932865	7801.421333	14.380928	-0.058812	4.757610
286.119216	7793.365538	14.385933	-0.058842	4.755227
286.056301	7785.284103	14.390938	-0.058825	4.752835
286.125647	7777.326540	14.395943	-0.058833	4.750479
286.178718	7769.363218	14.400947	-0.058838	4.748120
286.080590	7761.312438	14.405952	-0.058815	4.745735
285.757079	7753.306152	14.410957	-0.058750	4.743362
285.972638	7745.348377	14.415962	-0.058785	4.741001
285.786813	7737.330844	14.420967	-0.058745	4.738622
285.750168	7729.348586	14.425971	-0.058733	4.736251
285.842768	7721.341362	14.430976	-0.058746	4.733872
285.723766	7713.333653	14.435981	-0.058718	4.731492
285.562725	7705.308571	14.440986	-0.058683	4.729106
285.464424	7697.307173	14.445991	-0.058660	4.726726
285.508837	7689.287263	14.450995	-0.058663	4.724338
285.288020	7681.334636	14.456000	-0.058617	4.721970
285.225885	7673.359444	14.461005	-0.058601	4.719593
285.268016	7665.370511	14.466010	-0.058604	4.717211
285.205205	7657.334344	14.471015	-0.058587	4.714814
285.274242	7649.307759	14.476019	-0.058595	4.712418
285.350624	7641.256040	14.481024	-0.058604	4.710014
285.245302	7633.307012	14.486029	-0.058579	4.707639
285.143379	7625.270187	14.491034	-0.058555	4.705237
284.999775	7617.270539	14.496039	-0.058524	4.702845
285.201417	7609.366700	14.501043	-0.058556	4.700480
285.064200	7601.293940	14.506048	-0.058526	4.698063
285.110019	7593.284232	14.511053	-0.058529	4.695664
285.092104	7585.362452	14.516058	-0.058521	4.693290
284.967085	7577.232527	14.521063	-0.058492	4.690853
284.800788	7569.324014	14.526067	-0.058457	4.688480
284.880443	7561.265448	14.531072	-0.058466	4.686061
284.752375	7553.303035	14.536077	-0.058438	4.683671
284.587651	7545.356949	14.541082	-0.058402	4.681284
284.554976	7537.273661	14.546087	-0.058391	4.678854
284.712753	7529.327677	14.551091	-0.058415	4.676464
284.573629	7521.253061	14.556096	-0.058384	4.674034
284.373440	7513.132557	14.561101	-0.058342	4.671589
284.621126	7505.195299	14.566106	-0.058383	4.669198
284.574293	7497.197086	14.571111	-0.058369	4.666787
284.394316	7489.200190	14.576115	-0.058331	4.664376
284.276497	7481.281306	14.581120	-0.058304	4.661987
284.397037	7473.240641	14.586125	-0.058321	4.659560
284.222268	7465.297668	14.591130	-0.058284	4.657161
284.200289	7457.234645	14.596135	-0.058275	4.654725
284.042827	7449.242313	14.601139	-0.058240	4.652309
284.219742	7441.187646	14.606144	-0.058268	4.649872
284.159377	7433.230970	14.611149	-0.058252	4.647464
284.195607	7425.213920	14.616154	-0.058254	4.645036
284.202037	7417.275110	14.621159	-0.058250	4.642631
284.037551	7409.246063	14.626163	-0.058214	4.640198
283.820224	7401.246837	14.631168	-0.058169	4.637772
283.975754	7393.201744	14.636173	-0.058193	4.635330
283.958691	7385.231211	14.641178	-0.058185	4.632911
283.758272	7377.161547	14.646183	-0.058142	4.630460
283.802109	7369.201690	14.651187	-0.058146	4.628040
283.768621	7361.148271	14.656192	-0.058134	4.625591
283.577201	7353.232111	14.661197	-0.058094	4.623183
283.617212	7345.197645	14.666202	-0.058096	4.620737
283.711909	7337.212629	14.671207	-0.058109	4.618305
283.526260	7329.204632	14.676211	-0.058069	4.615865
283.391666	7321.168279	14.681216	-0.058039	4.613415
283.484565	7313.113062	14.686221	-0.058051	4.610958
283.410724	7305.204038	14.691226	-0.058033	4.608544
283.349760	7297.171449	14.696231	-0.058016	4.606091
283.477721	7289.248560	14.701235	-0.058035	4.603670
283.380248	7281.175467	14.706240	-0.058012	4.601202
283.438497	7273.222141	14.711245	-0.058018	4.598769
283.129098	7265.181101	14.716250	-0.057955	4.596309
283.185472	7257.104788	14.721255	-0.057961	4.593836
283.189963	7249.128579	14.726259	-0.057957	4.591392
282.786212	7241.128222	14.731264	-0.057876	4.588940
282.742760	7233.114840	14.736269	-0.057863	4.586482
282.869794	7225.135162	14.741274	-0.057882	4.584033
282.649223	7217.119339	14.746279	-0.057836	4.581572
282.753105	7209.189878	14.751283	-0.057850	4.579137
282.642472	7201.171443	14.756288	-0.057825	4.576672
282.076616	7193.168185	14.761293	-0.057714	4.574211
282.257981	7185.129693	14.766298	-0.057743	4.571737
282.637854	7177.067750	14.771303	-0.057809	4.569256
282.702771	7169.118096	14.776307	-0.057816	4.566807
282.472318	7161.118656	14.781312	-0.057768	4.564342
282.385784	7153.153654	14.786317	-0.057747	4.561886
282.277316	7145.130318	14.791322	-0.057722	4.559410
282.348904	7137.168517	14.796327	-0.057730	4.556953
282.440462	7129.137161	14.801331	-0.057742	4.554472
282.241016	7121.104013	14.806336	-0.057700	4.551990
282.190750	7113.106120	14.811341	-0.057686	4.549517
282.168501	7105.142770	14.816346	-0.057676	4.547053
282.156014	7097.069772	14.821351	-0.057669	4.544554
282.208584	7089.167255	14.826355	-0.057674	4.542107
281.912645	7081.120359	14.831360	-0.057614	4.539613
282.016584	7073.166864	14.836365	-0.057628	4.537147
282.094600	7065.120181	14.841370	-0.057638	4.534651
281.868529	7057.081366	14.846375	-0.057591	4.532156
281.787581	7049.099623	14.851379	-0.057571	4.529677
281.759172	7041.137085	14.856384	-0.057560	4.527203
281.781754	7033.067210	14.861389	-0.057559	4.524694
281.566902	7025.176710	14.866394	-0.057514	4.522239
281.551994	7017.091884	14.871399	-0.057507	4.519723
281.709149	7009.173920	14.876403	-0.057531	4.517257
281.504558	7001.091151	14.881408	-0.057488	4.514738
281.396297	6993.001360	14.886413	-0.057463	4.512216
281.348917	6985.039818	14.891418	-0.057449	4.509733
281.179754	6977.044506	14.896423	-0.057412	4.507237
281.256776	6969.086975	14.901427	-0.057422	4.504752
281.200632	6961.121774	14.906432	-0.057406	4.502263
281.169242	6953.023052	14.911437	-0.057395	4.499731
281.105389	6945.134699	14.916442	-0.057379	4.497264
281.240209	6937.048733	14.921447	-0.057399	4.494733
281.242493	6929.081943	14.926451	-0.057394	4.492238
281.011806	6921.044768	14.931456	-0.057346	4.489720
280.885517	6913.068084	14.936461	-0.057318	4.487219
281.130812	6905.043005	14.941466	-0.057358	4.484702
280.879209	6897.053502	14.946471	-0.057306	4.482194
280.985365	6889.050497	14.951475	-0.057321	4.479681
280.768915	6881.122418	14.956480	-0.057276	4.477189
280.719742	6873.059303	14.961485	-0.057262	4.474654
280.841618	6865.033894	14.966490	-0.057279	4.472130
280.632999	6857.024098	14.971495	-0.057236	4.469608
280.610190	6849.055736	14.976499	-0.057226	4.467099
280.535179	6841.031971	14.981504	-0.057207	4.464570
280.498401	6833.043086	14.986509	-0.057195	4.462052
280.521087	6825.048221	14.991514	-0.057195	4.459530
280.441510	6817.049075	14.996519	-0.057175	4.457004
280.492934	6808.994776	15.001523	-0.057179	4.454461
280.526942	6800.983777	15.006528	-0.057181	4.451930
280.378173	6793.000109	15.011533	-0.057148	4.449405
280.223023	6785.050709	15.016538	-0.057114	4.446890
280.209010	6777.032259	15.021543	-0.057107	4.444351
280.442076	6769.072644	15.026547	-0.057145	4.441831
280.387884	6761.021433	15.031552	-0.057130	4.439280
280.107162	6753.050482	15.036557	-0.057073	4.436751
280.123023	6745.037235	15.041562	-0.057071	4.434209
280.304340	6736.944899	15.046567	-0.057099	4.431641
280.075251	6728.990174	15.051571	-0.057052	4.429113
280.069608	6720.975320	15.056576	-0.057046	4.426566
280.040873	6712.993858	15.061581	-0.057035	4.424028
279.994216	6704.982902	15.066586	-0.057022	4.421479
279.774781	6696.972072	15.071591	-0.056976	4.418927
279.872725	6688.972376	15.076595	-0.056989	4.416379
279.766430	6680.986970	15.081600	-0.056964	4.413834
279.518573	6672.982778	15.086605	-0.056913	4.411280
279.699360	6664.982071	15.091610	-0.056942	4.408728
279.474335	6656.966416	15.096615	-0.056895	4.406167
279.447333	6649.006332	15.101619	-0.056885	4.403624
279.551236	6640.988377	15.106624	-0.056899	4.401062
279.541027	6633.020694	15.111629	-0.056892	4.398513
279.494240	6625.031869	15.116634	-0.056879	4.395956
279.389022	6616.970653	15.121639	-0.056854	4.393374
279.341481	6608.950334	15.126643	-0.056840	4.390804
279.310951	6600.957832	15.131648	-0.056829	4.388242
279.317686	6592.939257	15.136653	-0.056826	4.385670
279.292627	6585.060098	15.141658	-0.056816	4.383140
279.160083	6576.991942	15.146663	-0.056786	4.380549
279.144262	6569.025740	15.151667	-0.056778	4.377988
279.141986	6560.992154	15.156672	-0.056773	4.375405
279.021892	6553.011896	15.161677	-0.056746	4.372837
278.873156	6544.981616	15.166682	-0.056713	4.370251
278.722496	6536.984288	15.171687	-0.056680	4.367674
278.775914	6528.989112	15.176691	-0.056685	4.365098
278.802282	6521.042677	15.181696	-0.056685	4.362535
278.842356	6512.990398	15.186701	-0.056687	4.359937
278.870999	6505.052349	15.191706	-0.056688	4.357374
278.696135	6496.972013	15.196711	-0.056650	4.354763
278.565580	6488.896742	15.201715	-0.056621	4.352151
278.582176	6480.897904	15.206720	-0.056619	4.349564
278.657826	6472.913310	15.211725	-0.056628	4.346980
278.586082	6464.951694	15.216730	-0.056609	4.344402
278.469733	6456.979333	15.221735	-0.056583	4.341818
278.509618	6448.950953	15.226739	-0.056585	4.339215
278.510168	6441.008009	15.231744	-0.056580	4.336638
278.365915	6432.954431	15.236749	-0.056548	4.334023
278.340318	6424.966801	15.241754	-0.056539	4.331428
278.176822	6416.894601	15.246759	-0.056503	4.328803
278.203245	6408.947261	15.251763	-0.056503	4.326219
278.100631	6400.980493	15.256768	-0.056479	4.323626
278.220268	6392.928579	15.261773	-0.056496	4.321005
278.197474	6384.978407	15.266778	-0.056487	4.318414
278.063991	6376.946351	15.271783	-0.056457	4.315795
278.033874	6368.962929	15.276787	-0.056447	4.313191
278.171685	6360.928103	15.281792	-0.056467	4.310569
278.022036	6352.926408	15.286797	-0.056434	4.307955
278.090193	6344.926723	15.291802	-0.056442	4.305341
277.875266	6336.960156	15.296807	-0.056397	4.302734
277.879819	6328.943960	15.301811	-0.056393	4.300112
277.874865	6320.971963	15.306816	-0.056387	4.297502
277.646321	6312.913721	15.311821	-0.056339	4.294860
277.784395	6304.923467	15.316826	-0.056360	4.292242
277.583011	6296.897428	15.321831	-0.056318	4.289608
277.536290	6288.957407	15.326835	-0.056304	4.287002
277.608035	6280.920591	15.331840	-0.056312	4.284363
277.465968	6272.938457	15.336845	-0.056281	4.281739
277.431964	6264.942541	15.341850	-0.056270	4.279110
277.472829	6256.933613	15.346855	-0.056272	4.276475
277.421539	6248.921442	15.351859	-0.056258	4.273837
277.195017	6240.892045	15.356864	-0.056210	4.271190
277.334414	6232.868085	15.361869	-0.056231	4.268546
277.513489	6224.877387	15.366874	-0.056260	4.265912
277.042294	6216.902323	15.371879	-0.056167	4.263276
277.236083	6208.906944	15.376883	-0.056198	4.260638
277.219398	6200.940740	15.381888	-0.056190	4.258005
276.970622	6192.907134	15.386893	-0.056139	4.255347
276.958988	6184.942284	15.391898	-0.056132	4.252712
276.740078	6176.886009	15.396903	-0.056086	4.250043
276.546150	6168.952940	15.401907	-0.056045	4.247413
276.738466	6160.862047	15.406912	-0.056075	4.244733
276.724633	6152.926634	15.411917	-0.056068	4.242100
276.728713	6144.918564	15.416922	-0.056064	4.239443
276.337953	6136.978902	15.421927	-0.055986	4.236802
276.463786	6128.930633	15.426931	-0.056004	4.234129
276.486962	6120.878036	15.431936	-0.056004	4.231452
276.499741	6112.891794	15.436941	-0.056001	4.228795
276.575241	6104.912565	15.441946	-0.056010	4.226139
276.507889	6096.916128	15.446951	-0.055993	4.223474
276.392565	6088.957967	15.451955	-0.055966	4.220820
276.430293	6080.962128	15.456960	-0.055968	4.218153
276.245157	6072.934742	15.461965	-0.055929	4.215472
276.205241	6064.973747	15.466970	-0.055916	4.212813
276.065576	6056.896513	15.471975	-0.055885	4.210112
276.090719	6048.985802	15.476979	-0.055885	4.207467
276.012941	6040.914296	15.481984	-0.055865	4.204765
275.979891	6032.967853	15.486989	-0.055854	4.202104
275.801076	6024.990779	15.491994	-0.055816	4.199429
275.729470	6016.959783	15.496999	-0.055798	4.196736
275.952716	6008.901770	15.502003	-0.055834	4.194034
275.755575	6000.823594	15.507008	-0.055792	4.191320
275.507788	5992.859138	15.512013	-0.055741	4.188642
275.437567	5984.866535	15.517018	-0.055723	4.185955
275.424725	5976.872675	15.522023	-0.055716	4.183266
275.417479	5968.911609	15.527027	-0.055710	4.180586
275.405043	5960.928949	15.532032	-0.055702	4.177898
275.405769	5952.876010	15.537037	-0.055697	4.175184
275.376741	5944.925513	15.542042	-0.055687	4.172502
275.387645	5936.861405	15.547047	-0.055684	4.169781
275.226718	5928.960620	15.552051	-0.055649	4.167112
275.129151	5920.899422	15.557056	-0.055626	4.164387
275.081421	5912.948070	15.562061	-0.055612	4.161698
275.326379	5904.951666	15.567066	-0.055653	4.158995
274.968845	5896.913010	15.572071	-0.055581	4.156269
275.054016	5888.857674	15.577075	-0.055592	4.153541
274.804593	5880.866680	15.582080	-0.055540	4.150830
274.816524	5872.883256	15.587085	-0.055538	4.148122
274.871455	5864.882444	15.592090	-0.055543	4.145406
274.801270	5856.916849	15.597095	-0.055525	4.142700
274.782426	5848.901478	15.602099	-0.055516	4.139975
274.603731	5840.919849	15.607104	-0.055478	4.137259
274.675299	5832.896355	15.612109	-0.055486	4.134529
274.765972	5824.915961	15.617114	-0.055498	4.131812
274.597824	5816.870182	15.622119	-0.055462	4.129068
274.504161	5808.898588	15.627123	-0.055439	4.126348
274.577679	5800.908993	15.632128	-0.055448	4.123623
274.492906	5792.897395	15.637133	-0.055427	4.120886
274.576677	5784.935357	15.642138	-0.055438	4.118167
274.205126	5776.911893	15.647143	-0.055364	4.115419
274.289785	5768.875601	15.652147	-0.055375	4.112670
274.297167	5760.882106	15.657152	-0.055371	4.109933
274.262570	5752.853573	15.662157	-0.055359	4.107182
274.329414	5744.884968	15.667162	-0.055367	4.104451
274.257225	5736.893131	15.672167	-0.055349	4.101708
274.173694	5728.930735	15.677171	-0.055328	4.098974
274.279344	5720.930281	15.682176	-0.055343	4.096227
274.120913	5712.907860	15.687181	-0.055308	4.093467
273.893769	5704.898962	15.692186	-0.055261	4.090709
273.795165	5696.901565	15.697191	-0.055237	4.087955
273.981040	5688.906901	15.702195	-0.055267	4.085203
273.500222	5680.963956	15.707200	-0.055173	4.082459
273.452091	5672.887726	15.712205	-0.055159	4.079673
273.544574	5664.981576	15.717210	-0.055171	4.076945
273.612998	5656.905427	15.722215	-0.055179	4.074156
273.769128	5648.906296	15.727219	-0.055203	4.071394
273.669214	5640.931634	15.732224	-0.055179	4.068634
273.457457	5632.919964	15.737229	-0.055135	4.065858
273.367486	5624.993725	15.742234	-0.055113	4.063112
273.186525	5616.926140	15.747239	-0.055074	4.060313
273.287020	5608.968990	15.752243	-0.055088	4.057555
273.470398	5600.939236	15.757248	-0.055117	4.054771
273.259518	5592.916522	15.762253	-0.055073	4.051982
273.250558	5584.928924	15.767258	-0.055066	4.049206
273.036002	5576.946250	15.772263	-0.055021	4.046426
273.039959	5568.965557	15.777267	-0.055017	4.043649
273.031361	5560.979221	15.782272	-0.055010	4.040868
272.956250	5552.946526	15.787277	-0.054991	4.038067
272.950486	5544.973825	15.792282	-0.054985	4.035287
272.936229	5536.845117	15.797287	-0.054978	4.032450
272.730702	5528.842793	15.802291	-0.054934	4.029652
272.726682	5520.895648	15.807296	-0.054929	4.026875
272.582402	5512.879634	15.812301	-0.054897	4.024069
272.708041	5504.938914	15.817306	-0.054915	4.021292
272.739986	5496.918531	15.822311	-0.054916	4.018484
272.439309	5488.930537	15.827315	-0.054855	4.015680
272.422719	5480.914610	15.832320	-0.054847	4.012869
272.598172	5472.880853	15.837325	-0.054875	4.010052
272.628144	5464.945225	15.842330	-0.054875	4.007266
272.479066	5456.900406	15.847335	-0.054842	4.004436
272.420439	5448.986038	15.852339	-0.054827	4.001652
272.378665	5440.934575	15.857344	-0.054814	3.998818
272.172237	5432.950215	15.862349	-0.054770	3.996003
272.250975	5424.943798	15.867354	-0.054780	3.993183
272.194347	5416.892442	15.872359	-0.054764	3.990342
272.149816	5408.917933	15.877363	-0.054751	3.987527
272.115141	5400.889430	15.882368	-0.054740	3.984691
272.031483	5392.948360	15.887373	-0.054719	3.981883
272.071748	5384.983459	15.892378	-0.054722	3.979067
271.933203	5376.968004	15.897383	-0.054691	3.976228
271.910512	5368.936271	15.902387	-0.054682	3.973383
271.781206	5360.931079	15.907392	-0.054653	3.970543
271.775962	5352.914484	15.912397	-0.054647	3.967700
271.754483	5344.940449	15.917402	-0.054638	3.964869
271.722829	5336.976994	15.922407	-0.054627	3.962040
271.767660	5328.972634	15.927411	-0.054630	3.959195
271.563788	5321.013816	15.932416	-0.054587	3.956361
271.599833	5312.952120	15.937421	-0.054589	3.953492
271.447329	5304.928010	15.942426	-0.054555	3.950631
271.341906	5296.932924	15.947431	-0.054531	3.947779
271.277640	5288.967938	15.952435	-0.054514	3.944936
271.452781	5280.993708	15.957440	-0.054541	3.942092
271.279970	5272.970348	15.962445	-0.054504	3.939223
271.125951	5264.997395	15.967450	-0.054471	3.936370
271.154628	5256.989992	15.972455	-0.054471	3.933505
271.090168	5248.998201	15.977459	-0.054454	3.930643
270.984246	5241.048271	15.982464	-0.054429	3.927792
270.791334	5232.959622	15.987469	-0.054388	3.924888
271.010125	5225.014087	15.992474	-0.054424	3.922041
270.771070	5216.987483	15.997479	-0.054375	3.919155
270.830890	5209.034492	16.002483	-0.054381	3.916298
270.893383	5201.006447	16.007488	-0.054387	3.913412
270.711048	5192.949787	16.012493	-0.054348	3.910509
270.650734	5185.008280	16.017498	-0.054332	3.907648
270.556180	5176.961794	16.022503	-0.054310	3.904746
270.514447	5169.033725	16.027507	-0.054297	3.901885
270.406899	5161.017156	16.032512	-0.054272	3.898990
270.499973	5152.964346	16.037517	-0.054284	3.896082
270.374238	5145.009058	16.042522	-0.054256	3.893204
270.273088	5136.983392	16.047527	-0.054232	3.890299
270.327450	5129.017774	16.052531	-0.054237	3.887416
270.505901	5120.980959	16.057536	-0.054265	3.884508
270.345193	5113.025476	16.062541	-0.054230	3.881620
270.112273	5105.057412	16.067546	-0.054182	3.878724
269.899783	5097.000651	16.072551	-0.054137	3.875795
270.094044	5088.833274	16.077555	-0.054168	3.872830
269.823478	5080.834872	16.082560	-0.054113	3.869916
269.756758	5072.860067	16.087565	-0.054096	3.867012
269.882477	5064.964121	16.092570	-0.054114	3.864139
269.764825	5056.974886	16.097575	-0.054087	3.861225
269.953329	5049.000080	16.102579	-0.054117	3.858319
269.927010	5041.001770	16.107584	-0.054107	3.855399
269.725871	5032.980569	16.112589	-0.054065	3.852465
269.578518	5024.996792	16.117594	-0.054033	3.849543
269.484765	5016.998309	16.122599	-0.054010	3.846614
269.762239	5009.000974	16.127603	-0.054057	3.843691
269.641273	5001.022991	16.132608	-0.054029	3.840765
269.343600	4993.044725	16.137613	-0.053969	3.837834
269.452785	4985.059523	16.142618	-0.053984	3.834905
269.234261	4977.020413	16.147623	-0.053938	3.831948
269.054490	4969.032146	16.152627	-0.053900	3.829008
269.191593	4961.034917	16.157632	-0.053921	3.826069
269.319419	4953.030738	16.162637	-0.053939	3.823125
269.288496	4945.075499	16.167642	-0.053929	3.820193
269.134820	4937.079156	16.172647	-0.053895	3.817242
269.068868	4929.049419	16.177651	-0.053878	3.814277
269.095095	4921.038459	16.182656	-0.053878	3.811320
268.948949	4913.076490	16.187661	-0.053845	3.808374
268.970278	4905.102715	16.192666	-0.053844	3.805425
268.677151	4897.135494	16.197671	-0.053785	3.802470
268.827518	4889.113630	16.202675	-0.053808	3.799502
268.802631	4881.147685	16.207680	-0.053798	3.796548
268.793324	4873.086957	16.212685	-0.053791	3.793557
268.651269	4865.071429	16.217690	-0.053760	3.790578
268.551697	4857.058948	16.222695	-0.053736	3.787598
268.817088	4849.048192	16.227699	-0.053781	3.784625
268.539639	4841.122531	16.232704	-0.053724	3.781669
268.602172	4833.060792	16.237709	-0.053731	3.778667
268.501188	4825.114749	16.242714	-0.053707	3.775703
268.287030	4817.115641	16.247719	-0.053662	3.772714
268.264007	4809.081481	16.252723	-0.053653	3.769714
268.249738	4801.120858	16.257728	-0.053645	3.766739
268.282409	4793.102800	16.262733	-0.053646	3.763741
268.208319	4785.145080	16.267738	-0.053628	3.760761
267.938605	4777.150539	16.272743	-0.053572	3.757760
268.057998	4769.100623	16.277747	-0.053590	3.754746
268.055742	4761.121089	16.282752	-0.053584	3.751752
267.833537	4753.070755	16.287757	-0.053538	3.748724
267.998179	4745.102178	16.292762	-0.053563	3.745734
267.916041	4737.138455	16.297767	-0.053543	3.742737
267.842770	4729.126711	16.302771	-0.053525	3.739720
267.789625	4721.217989	16.307776	-0.053510	3.736739
267.798896	4713.126304	16.312781	-0.053506	3.733689
267.701987	4705.138821	16.317786	-0.053483	3.730673
267.349656	4697.155598	16.322791	-0.053413	3.727651
267.569623	4689.098605	16.327795	-0.053449	3.724611
267.651200	4681.202008	16.332800	-0.053459	3.721626
267.490431	4673.158784	16.337805	-0.053424	3.718578
267.536742	4665.195651	16.342810	-0.053428	3.715563
267.466938	4657.098988	16.347815	-0.053410	3.712491
267.226300	4649.105451	16.352819	-0.053360	3.709452
267.174423	4641.178858	16.357824	-0.053345	3.706441
267.166464	4633.136871	16.362829	-0.053339	3.703384
267.270661	4625.162433	16.367834	-0.053353	3.700353
266.946823	4617.219565	16.372839	-0.053288	3.697321
266.938523	4609.215495	16.377843	-0.053281	3.694271
266.779366	4601.205713	16.382848	-0.053247	3.691213
266.742409	4593.207796	16.387853	-0.053235	3.688160
266.711832	4585.213658	16.392858	-0.053224	3.685106
266.835996	4577.245448	16.397863	-0.053242	3.682063
266.590331	4569.250905	16.402867	-0.053191	3.678998
266.487150	4561.274153	16.407872	-0.053167	3.675941
266.585695	4553.215067	16.412877	-0.053181	3.672854
266.586895	4545.213898	16.417882	-0.053176	3.669786
266.387407	4537.244923	16.422887	-0.053134	3.666721
266.634175	4529.225422	16.427891	-0.053175	3.663646
266.524936	4521.235473	16.432896	-0.053149	3.660571
266.431552	4513.273937	16.437901	-0.053127	3.657505
266.402969	4505.263738	16.442906	-0.053117	3.654419
266.164175	4497.259891	16.447911	-0.053067	3.651327
266.252140	4489.252218	16.452915	-0.053078	3.648240
266.023679	4481.275119	16.457920	-0.053031	3.645153
266.103076	4473.275117	16.462925	-0.053041	3.642063
266.145488	4465.295685	16.467930	-0.053044	3.638978
265.834207	4457.313286	16.472935	-0.052981	3.635879
265.870046	4449.243211	16.477939	-0.052982	3.632753
266.119063	4441.224989	16.482944	-0.053024	3.629650
265.910132	4433.266741	16.487949	-0.052980	3.626556
265.873158	4425.296288	16.492954	-0.052968	3.623458
265.802212	4417.278840	16.497959	-0.052950	3.620339
265.741627	4409.310121	16.502963	-0.052933	3.617237
265.718388	4401.315227	16.507968	-0.052924	3.614122
265.652755	4393.276563	16.512973	-0.052907	3.610987
265.759119	4385.319261	16.517978	-0.052922	3.607885
265.543893	4377.325800	16.522983	-0.052877	3.604758
265.551754	4369.367591	16.527987	-0.052873	3.601648
265.494119	4361.401735	16.532992	-0.052857	3.598530
265.197259	4353.400760	16.537997	-0.052797	3.595389
265.316999	4345.371778	16.543002	-0.052814	3.592246
265.330540	4337.354945	16.548007	-0.052812	3.589102
265.241333	4329.367570	16.553011	-0.052790	3.585964
265.124463	4321.401920	16.558016	-0.052764	3.582832
265.333121	4313.365185	16.563021	-0.052797	3.579677
265.240414	4305.434825	16.568026	-0.052775	3.576553
264.995509	4297.402803	16.573031	-0.052725	3.573382
264.959130	4289.396976	16.578035	-0.052713	3.570225
265.131479	4281.434516	16.583040	-0.052740	3.567087
264.889440	4273.422215	16.588045	-0.052690	3.563916
264.870138	4265.462490	16.593050	-0.052681	3.560768
264.871743	4257.457815	16.598055	-0.052677	3.557601
264.902702	4249.404540	16.603059	-0.052677	3.554413
264.809506	4241.351863	16.608064	-0.052655	3.551218
264.760668	4233.350403	16.613069	-0.052641	3.548042
264.561271	4225.400264	16.618074	-0.052599	3.544879
264.691437	4217.416414	16.623079	-0.052618	3.541709
264.565119	4209.440666	16.628083	-0.052590	3.538533
264.504219	4201.442192	16.633088	-0.052573	3.535346
264.471370	4193.430859	16.638093	-0.052562	3.532152
264.519019	4185.452057	16.643098	-0.052566	3.528971
264.381897	4177.441936	16.648103	-0.052535	3.525769
264.353705	4169.484843	16.653107	-0.052525	3.522588
264.220192	4161.483608	16.658112	-0.052495	3.519384
264.110912	4153.512836	16.663117	-0.052470	3.516189
264.176869	4145.497915	16.668122	-0.052477	3.512980
263.971069	4137.446381	16.673127	-0.052434	3.509744
263.985151	4129.492100	16.678131	-0.052432	3.506551
263.980007	4121.521681	16.683136	-0.052426	3.503348
263.853988	4113.520490	16.688141	-0.052397	3.500126
263.795262	4105.559544	16.693146	-0.052381	3.496920
263.816652	4097.553295	16.698151	-0.052380	3.493694
263.623494	4089.564808	16.703155	-0.052339	3.490466
263.496771	4081.584847	16.708160	-0.052311	3.487241
263.494568	4073.567917	16.713165	-0.052305	3.484002
263.466268	4065.596743	16.718170	-0.052295	3.480777
263.337186	4057.624645	16.723175	-0.052266	3.477546
263.250704	4049.629736	16.728179	-0.052245	3.474304
263.303710	4041.587545	16.733184	-0.052250	3.471044
263.128984	4033.572321	16.738189	-0.052212	3.467784
263.312765	4025.584861	16.743194	-0.052241	3.464544
263.131073	4017.621375	16.748199	-0.052203	3.461300
263.078963	4009.633725	16.753203	-0.052188	3.458046
263.190874	4001.618397	16.758208	-0.052204	3.454784
263.146922	3993.620697	16.763213	-0.052191	3.451520
263.224014	3985.635456	16.768218	-0.052200	3.448263
263.094891	3977.615414	16.773223	-0.052171	3.444981
262.892494	3969.714230	16.778227	-0.052128	3.441743
263.056378	3961.677596	16.783232	-0.052154	3.438458
262.719872	3953.686577	16.788237	-0.052086	3.435172
262.712957	3945.668394	16.793242	-0.052080	3.431883
262.799678	3937.671610	16.798247	-0.052091	3.428602
262.695181	3929.659231	16.803251	-0.052067	3.425306
262.616289	3921.726113	16.808256	-0.052047	3.422039
262.408733	3913.726982	16.813261	-0.052003	3.418738
262.620211	3905.730214	16.818266	-0.052038	3.415449
262.572432	3897.703291	16.823271	-0.052024	3.412136
262.459358	3889.723553	16.828275	-0.051998	3.408837
262.534404	3881.746687	16.833280	-0.052007	3.405542
262.404918	3873.747624	16.838285	-0.051978	3.402227
262.383853	3865.797934	16.843290	-0.051969	3.398934
262.244315	3857.811589	16.848295	-0.051938	3.395618
262.189441	3849.723072	16.853299	-0.051922	3.392259
262.136703	3841.758097	16.858304	-0.051908	3.388949
261.971561	3833.744277	16.863309	-0.051872	3.385611
262.160992	3825.803995	16.868314	-0.051902	3.382312
262.100750	3817.797188	16.873319	-0.051886	3.378974
261.972305	3809.822762	16.878323	-0.051857	3.375644
261.866377	3801.829708	16.883328	-0.051832	3.372304
261.830646	3793.818540	16.888333	-0.051821	3.368955
261.580115	3785.844725	16.893338	-0.051769	3.365610
261.436374	3777.869155	16.898343	-0.051737	3.362266
261.456703	3769.896581	16.903347	-0.051736	3.358925
261.596792	3761.891979	16.908352	-0.051757	3.355572
261.538489	3753.847618	16.913357	-0.051741	3.352191
261.465900	3745.872748	16.918362	-0.051723	3.348836
261.426256	3737.886769	16.923367	-0.051710	3.345474
261.281037	3729.914215	16.928371	-0.051678	3.342110
261.198240	3721.936981	16.933376	-0.051658	3.338743
261.299142	3713.923139	16.938381	-0.051672	3.335364
261.142020	3705.938233	16.943386	-0.051638	3.331985
261.040012	3697.933117	16.948391	-0.051614	3.328595
261.050715	3689.933777	16.953395	-0.051611	3.325209
261.241508	3681.971065	16.958400	-0.051641	3.321841
260.891365	3673.984155	16.963405	-0.051571	3.318440
260.999742	3665.990448	16.968410	-0.051586	3.315049
260.757303	3657.979867	16.973415	-0.051536	3.311634
260.764612	3649.962306	16.978419	-0.051532	3.308223
260.821246	3641.976504	16.983424	-0.051538	3.304823
260.543598	3634.025493	16.988429	-0.051481	3.301422
260.645802	3626.051383	16.993434	-0.051495	3.298021
260.614284	3618.026484	16.998439	-0.051484	3.294591
260.685393	3610.029286	17.003443	-0.051493	3.291173
260.520940	3602.065726	17.008448	-0.051457	3.287756
260.233060	3594.058948	17.013453	-0.051398	3.284313
260.263157	3586.110058	17.018458	-0.051399	3.280903
260.435310	3578.121087	17.023463	-0.051426	3.277478
260.314349	3570.104329	17.028467	-0.051399	3.274026
260.339292	3562.101067	17.033472	-0.051398	3.270582
260.306170	3554.107848	17.038477	-0.051387	3.267136
260.291612	3546.125018	17.043482	-0.051379	3.263692
260.220103	3538.126164	17.048487	-0.051361	3.260235
259.879596	3530.192751	17.053491	-0.051293	3.256792
260.170051	3522.154209	17.058496	-0.051342	3.253325
259.946510	3514.141466	17.063501	-0.051295	3.249845
259.910587	3506.207321	17.068506	-0.051283	3.246402
260.050070	3498.203729	17.073511	-0.051304	3.242933
260.012030	3490.193348	17.078515	-0.051292	3.239450
259.721245	3482.290883	17.083520	-0.051233	3.236000
259.638094	3474.197308	17.088525	-0.051213	3.232472
259.639559	3466.187807	17.093530	-0.051208	3.228980
259.559204	3458.193835	17.098535	-0.051188	3.225487
259.419429	3450.230503	17.103539	-0.051157	3.222002
259.610612	3442.238660	17.108544	-0.051188	3.218513
259.265141	3434.279040	17.113549	-0.051118	3.215014
259.422573	3426.282007	17.118554	-0.051143	3.211514
259.380473	3418.293804	17.123559	-0.051130	3.208007
259.178972	3410.278886	17.128563	-0.051087	3.204477
259.200276	3402.356955	17.133568	-0.051086	3.200993
259.014877	3394.367441	17.138573	-0.051047	3.197468
259.022705	3386.373554	17.143578	-0.051043	3.193944
258.979653	3378.343099	17.148583	-0.051030	3.190399
258.922571	3370.376600	17.153587	-0.051015	3.186877
259.122205	3362.380455	17.158592	-0.051047	3.183348
259.075724	3354.379146	17.163597	-0.051033	3.179804
258.878050	3346.438505	17.168602	-0.050991	3.176276
258.671452	3338.435219	17.173607	-0.050948	3.172715
258.779295	3330.384234	17.178611	-0.050963	3.169143
258.731189	3322.450538	17.183616	-0.050949	3.165612
258.731846	3314.462170	17.188621	-0.050944	3.162055
258.720511	3306.486747	17.193626	-0.050937	3.158500
258.579479	3298.508359	17.198631	-0.050906	3.154933
258.469857	3290.500410	17.203635	-0.050880	3.151351
258.286359	3282.521340	17.208640	-0.050841	3.147774
258.261005	3274.501937	17.213645	-0.050832	3.144182
258.326034	3266.535121	17.218650	-0.050839	3.140613
258.273138	3258.555455	17.223655	-0.050824	3.137029
258.095684	3250.556134	17.228659	-0.050786	3.133427
258.097621	3242.546465	17.233664	-0.050781	3.129824
257.930103	3234.582729	17.238669	-0.050745	3.126230
258.027278	3226.608458	17.243674	-0.050758	3.122639
257.700548	3218.660857	17.248679	-0.050692	3.119036
257.735442	3210.666218	17.253683	-0.050694	3.115425
257.826687	3202.634578	17.258688	-0.050706	3.111795
257.719655	3194.620195	17.263693	-0.050681	3.108160
257.853485	3186.645004	17.268698	-0.050701	3.104549
257.927350	3178.683615	17.273703	-0.050710	3.100937
257.734833	3170.721624	17.278707	-0.050669	3.097309
257.489273	3162.757218	17.283712	-0.050618	3.093673
257.280045	3154.734301	17.288717	-0.050574	3.090008
257.408937	3146.754839	17.293722	-0.050593	3.086374
257.119749	3138.800047	17.298727	-0.050534	3.082727
257.084065	3130.782916	17.303731	-0.050523	3.079060
257.184867	3122.835205	17.308736	-0.050536	3.075425
257.129215	3114.729531	17.313741	-0.050521	3.071708
257.061171	3106.758690	17.318746	-0.050503	3.068046
256.955762	3098.789645	17.323751	-0.050479	3.064380
256.872267	3090.832037	17.328755	-0.050458	3.060715
256.954797	3082.850172	17.333760	-0.050469	3.057043
256.744436	3074.866447	17.338765	-0.050424	3.053351
256.915851	3066.833890	17.343770	-0.050451	3.049651
256.857039	3058.882481	17.348775	-0.050435	3.045973
256.662382	3050.933067	17.353779	-0.050394	3.042284
256.807253	3042.947066	17.358784	-0.050416	3.038591
256.690479	3034.946523	17.363789	-0.050389	3.034873
256.647796	3026.960293	17.368794	-0.050377	3.031161
256.636294	3018.965218	17.373799	-0.050369	3.027443
256.484951	3010.983730	17.378803	-0.050336	3.023719
256.482029	3003.014830	17.383808	-0.050331	3.020003
256.290375	2995.060645	17.388813	-0.050290	3.016281
256.226599	2987.053002	17.393818	-0.050273	3.012535
256.313671	2979.030953	17.398823	-0.050284	3.008785
256.195665	2971.068256	17.403827	-0.050257	3.005048
256.068520	2963.149070	17.408832	-0.050229	3.001327
255.953223	2955.145539	17.413837	-0.050202	2.997562
255.981627	2947.148967	17.418842	-0.050203	2.993802
255.732446	2939.126056	17.423847	-0.050151	2.990012
255.807204	2931.126928	17.428851	-0.050160	2.986244
255.801606	2923.181374	17.433856	-0.050154	2.982493
255.627867	2915.198936	17.438861	-0.050117	2.978711
255.595577	2907.237435	17.443866	-0.050106	2.974941
255.569098	2899.224858	17.448871	-0.050096	2.971142
255.524585	2891.237613	17.453875	-0.050083	2.967350
255.683475	2883.250733	17.458880	-0.050107	2.963563
255.514094	2875.272976	17.463885	-0.050071	2.959759
255.528315	2867.323905	17.468890	-0.050068	2.955974
255.471239	2859.318082	17.473895	-0.050053	2.952152
255.230311	2851.332605	17.478899	-0.050003	2.948326
255.333814	2843.331649	17.483904	-0.050017	2.944506
255.284533	2835.359449	17.488909	-0.050003	2.940686
255.116499	2827.438441	17.493914	-0.049967	2.936879
255.067931	2819.427131	17.498919	-0.049953	2.933031
255.008629	2811.391179	17.503923	-0.049937	2.929165
255.166862	2803.442068	17.508928	-0.049961	2.925347
255.154835	2795.469984	17.513933	-0.049954	2.921504
255.047320	2787.518800	17.518938	-0.049929	2.917661
254.901969	2779.486729	17.523943	-0.049897	2.913772
254.845882	2771.430552	17.528947	-0.049881	2.909871
254.882802	2763.485769	17.533952	-0.049883	2.906023
254.687253	2755.521700	17.538957	-0.049842	2.902149
254.814251	2747.552174	17.543962	-0.049861	2.898284
254.783149	2739.558036	17.548967	-0.049850	2.894393
254.587344	2731.577465	17.553971	-0.049808	2.890495
254.466692	2723.629519	17.558976	-0.049781	2.886612
254.555617	2715.632083	17.563981	-0.049793	2.882710
254.388605	2707.658505	17.568986	-0.049756	2.878801
254.273038	2699.732171	17.573991	-0.049730	2.874913
254.326209	2691.687795	17.578995	-0.049735	2.870970
254.310723	2683.708466	17.584000	-0.049727	2.867051
254.055526	2675.735113	17.589005	-0.049674	2.863115
254.124868	2667.771391	17.594010	-0.049682	2.859197
254.078540	2659.793554	17.599015	-0.049669	2.855260
254.035631	2651.789719	17.604019	-0.049656	2.851305
254.105464	2643.827862	17.609024	-0.049664	2.847372
253.957461	2635.857411	17.614029	-0.049631	2.843417
253.985705	2627.883901	17.619034	-0.049632	2.839464
253.676665	2619.964634	17.624039	-0.049569	2.835514
253.642712	2611.916884	17.629043	-0.049558	2.831510
253.760236	2603.922239	17.634048	-0.049575	2.827536
253.626883	2595.942881	17.639053	-0.049545	2.823549
253.673868	2587.966831	17.644058	-0.049549	2.819568
253.553557	2580.018599	17.649063	-0.049521	2.815587
253.435787	2572.003519	17.654067	-0.049494	2.811566
253.334448	2564.054072	17.659072	-0.049470	2.807573
253.364788	2556.058036	17.664077	-0.049471	2.803559
253.351543	2548.104490	17.669082	-0.049464	2.799558
253.273118	2540.158048	17.674087	-0.049444	2.795550
253.238436	2532.123994	17.679091	-0.049433	2.791496
253.156952	2524.168171	17.684096	-0.049412	2.787472
253.136971	2516.177920	17.689101	-0.049404	2.783429
252.951117	2508.235734	17.694106	-0.049364	2.779394
252.983267	2500.239318	17.699111	-0.049365	2.775339
252.927802	2492.229750	17.704115	-0.049350	2.771266
252.784823	2484.298574	17.709120	-0.049318	2.767222
252.732966	2476.321311	17.714125	-0.049304	2.763154
252.705986	2468.354753	17.719130	-0.049294	2.759086
252.605764	2460.400587	17.724135	-0.049270	2.755015
252.807827	2452.264363	17.729139	-0.049303	2.750862
252.672409	2444.343605	17.734144	-0.049272	2.746794
252.576171	2436.374148	17.739149	-0.049249	2.742696
252.572948	2428.423904	17.744154	-0.049244	2.738609
252.534870	2420.454503	17.749159	-0.049232	2.734502
252.547870	2412.449924	17.754163	-0.049229	2.730375
252.380372	2404.518053	17.759168	-0.049193	2.726268
252.098661	2396.567737	17.764173	-0.049136	2.722138
252.227954	2388.601331	17.769178	-0.049155	2.718019
252.042325	2380.624845	17.774183	-0.049115	2.713869
252.013359	2372.596983	17.779187	-0.049105	2.709696
252.063602	2364.648178	17.784192	-0.049109	2.705562
251.920127	2356.664014	17.789197	-0.049078	2.701391
252.040311	2348.702537	17.794202	-0.049095	2.697242
252.000961	2340.722243	17.799207	-0.049083	2.693067
251.793991	2332.720259	17.804211	-0.049039	2.688864
251.566389	2324.804758	17.809216	-0.048992	2.684698
251.725633	2316.806382	17.814221	-0.049016	2.680506
251.715314	2308.862815	17.819226	-0.049010	2.676326
251.771875	2300.837744	17.824231	-0.049015	2.672101
251.389920	2292.882540	17.829235	-0.048939	2.667878
251.570087	2284.902104	17.834240	-0.048968	2.663670
251.327198	2276.937812	17.839245	-0.048917	2.659438
251.329344	2268.980655	17.844250	-0.048913	2.655218
251.293238	2260.979137	17.849255	-0.048901	2.650966
251.209726	2253.011503	17.854259	-0.048880	2.646721
251.266514	2245.048918	17.859264	-0.048886	2.642482
251.034106	2237.091803	17.864269	-0.048838	2.638220
250.903801	2229.139831	17.869274	-0.048809	2.633960
250.921577	2221.133096	17.874279	-0.048807	2.629674
250.674775	2213.171647	17.879283	-0.048756	2.625388
250.837444	2205.197875	17.884288	-0.048781	2.621115
250.717518	2197.229839	17.889293	-0.048754	2.616819
250.602585	2189.257262	17.894298	-0.048728	2.612514
250.603240	2181.269430	17.899303	-0.048723	2.608202
250.708301	2173.287343	17.904307	-0.048737	2.603893
250.713212	2165.355887	17.909312	-0.048733	2.599597
250.646181	2157.395023	17.914317	-0.048716	2.595273
250.476115	2149.268591	17.919322	-0.048679	2.590845
250.382589	2141.287840	17.924327	-0.048657	2.586494
250.282816	2133.355099	17.929331	-0.048633	2.582161
250.468267	2125.414318	17.934336	-0.048663	2.577836
250.275814	2117.463980	17.939341	-0.048622	2.573473
250.238600	2109.509460	17.944346	-0.048610	2.569110
250.170158	2101.555065	17.949351	-0.048592	2.564738
250.007147	2093.621070	17.954355	-0.048557	2.560364
249.911738	2085.683994	17.959360	-0.048534	2.555984
249.739283	2077.678735	17.964365	-0.048497	2.551555
249.727973	2069.696438	17.969370	-0.048490	2.547141
249.785054	2061.732551	17.974375	-0.048496	2.542735
249.704027	2053.773240	17.979379	-0.048476	2.538314
249.855809	2045.796014	17.984384	-0.048499	2.533891
249.636866	2037.824319	17.989389	-0.048453	2.529438
249.593917	2029.869251	17.994394	-0.048440	2.524999
249.528148	2021.929711	17.999399	-0.048423	2.520559
249.501074	2013.959954	18.004403	-0.048413	2.516097
249.513844	2005.976433	18.009408	-0.048410	2.511622
249.119614	1998.017659	18.014413	-0.048332	2.507123
249.294312	1990.035272	18.019418	-0.048360	2.502645
249.184556	1982.095619	18.024423	-0.048334	2.498162
249.106719	1974.130817	18.029427	-0.048315	2.493658
249.090390	1966.152383	18.034432	-0.048307	2.489144
248.963061	1958.188458	18.039437	-0.048278	2.484621
248.837140	1950.256503	18.044442	-0.048250	2.480108
248.844979	1942.304449	18.049447	-0.048246	2.475586
248.676133	1934.308562	18.054451	-0.048210	2.471017
248.726091	1926.351299	18.059456	-0.048214	2.466478
248.573160	1918.381611	18.064461	-0.048181	2.461908
248.445145	1910.456492	18.069466	-0.048152	2.457357
248.447531	1902.475859	18.074471	-0.048147	2.452776
248.484089	1894.477189	18.079475	-0.048149	2.448178
248.682096	1886.504308	18.084480	-0.048181	2.443599
248.564334	1878.569009	18.089485	-0.048154	2.439009
248.361422	1870.635361	18.094490	-0.048111	2.434404
248.249917	1862.596642	18.099495	-0.048085	2.429737
248.413145	1854.605197	18.104499	-0.048111	2.425110
248.261484	1846.699380	18.109504	-0.048078	2.420499
247.979474	1838.774563	18.114509	-0.048020	2.415858
248.030457	1830.786376	18.119514	-0.048025	2.411197
248.161663	1822.812293	18.124519	-0.048044	2.406542
247.796590	1814.899179	18.129523	-0.047971	2.401874
247.770167	1806.960389	18.134528	-0.047961	2.397209
247.764373	1798.973903	18.139533	-0.047955	2.392508
247.868964	1790.976496	18.144538	-0.047970	2.387801
247.679076	1783.049393	18.149543	-0.047930	2.383102
247.524312	1775.101998	18.154547	-0.047896	2.378385
247.637601	1767.134320	18.159552	-0.047912	2.373667
247.523356	1759.144947	18.164557	-0.047886	2.368909
247.347024	1751.236841	18.169562	-0.047848	2.364185
247.548424	1743.267736	18.174567	-0.047880	2.359445
247.167522	1735.355864	18.179571	-0.047804	2.354684
247.236534	1727.344148	18.184576	-0.047812	2.349888
247.253079	1719.374771	18.189581	-0.047810	2.345105
246.966867	1711.452978	18.194586	-0.047752	2.340315
246.934380	1703.502880	18.199591	-0.047741	2.335520
246.724193	1695.544433	18.204595	-0.047697	2.330694
246.732626	1687.587334	18.209600	-0.047694	2.325878
246.594941	1679.640608	18.214605	-0.047663	2.321046
246.752432	1671.679037	18.219610	-0.047687	2.316219
246.672951	1663.712251	18.224615	-0.047668	2.311359
246.787732	1655.730368	18.229619	-0.047684	2.306496
246.556421	1647.826579	18.234624	-0.047636	2.301641
246.330561	1639.907324	18.239629	-0.047589	2.296767
246.458642	1631.912568	18.244634	-0.047608	2.291866
246.318436	1623.967607	18.249639	-0.047577	2.286963
246.120114	1616.039927	18.254643	-0.047535	2.282055
246.415679	1608.068211	18.259648	-0.047585	2.277151
246.060797	1600.095215	18.264653	-0.047514	2.272180
245.964365	1592.106210	18.269658	-0.047491	2.267210
245.962653	1584.166017	18.274663	-0.047486	2.262268
245.734768	1576.241491	18.279667	-0.047438	2.257305
245.805927	1568.282334	18.284672	-0.047447	2.252336
245.611188	1560.341274	18.289677	-0.047405	2.247343
245.736775	1552.385844	18.294682	-0.047424	2.242359
245.811084	1544.447214	18.299687	-0.047433	2.237369
245.673768	1536.492456	18.304691	-0.047402	2.232340
245.532477	1528.565387	18.309696	-0.047371	2.227316
245.409904	1520.612571	18.314701	-0.047343	2.222267
245.396500	1512.681764	18.319706	-0.047336	2.217229
245.603624	1504.693952	18.324711	-0.047369	2.212164
245.270129	1496.770869	18.329715	-0.047302	2.207079
245.321501	1488.843838	18.334720	-0.047307	2.202015
245.167328	1480.922092	18.339725	-0.047273	2.196924
245.087250	1472.953741	18.344730	-0.047253	2.191798
244.959696	1465.001817	18.349735	-0.047225	2.186667
244.948826	1457.050685	18.354739	-0.047218	2.181534
244.883689	1449.132448	18.359744	-0.047200	2.176405
244.754963	1441.186140	18.364749	-0.047172	2.171241
244.728607	1433.228209	18.369754	-0.047162	2.166065
244.792049	1425.295911	18.374759	-0.047168	2.160903
244.727386	1417.369474	18.379763	-0.047152	2.155720
244.678323	1409.409657	18.384768	-0.047137	2.150504
244.561704	1401.469786	18.389773	-0.047111	2.145282
244.688645	1393.516391	18.394778	-0.047129	2.140061
244.431046	1385.630956	18.399783	-0.047077	2.134837
244.105114	1377.687539	18.404787	-0.047011	2.129554
244.238462	1369.730121	18.409792	-0.047031	2.124293
244.110249	1361.816753	18.414797	-0.047002	2.119023
244.162050	1353.856745	18.419802	-0.047007	2.113725
244.241595	1345.851932	18.424807	-0.047016	2.108388
244.014672	1337.937153	18.429811	-0.046969	2.103067
243.874105	1330.035416	18.434816	-0.046938	2.097750
243.839667	1322.088626	18.439821	-0.046927	2.092400
243.846208	1314.140745	18.444826	-0.046923	2.087039
243.644631	1306.252443	18.449831	-0.046880	2.081684
243.437967	1298.342546	18.454835	-0.046837	2.076300
243.651299	1290.355054	18.459840	-0.046872	2.070891
243.544516	1282.419322	18.464845	-0.046847	2.065471
243.397115	1274.523862	18.469850	-0.046815	2.060061
243.343308	1266.602348	18.474855	-0.046800	2.054627
243.436034	1258.618887	18.479859	-0.046812	2.049152
243.347479	1250.722363	18.484864	-0.046790	2.043703
243.017256	1242.844689	18.489869	-0.046724	2.038228
243.033096	1234.882234	18.494874	-0.046722	2.032715
243.025506	1226.922340	18.499879	-0.046716	2.027186
242.779831	1219.020535	18.504883	-0.046665	2.021658
242.801461	1211.110483	18.509888	-0.046664	2.016137
242.626272	1203.167623	18.514893	-0.046626	2.010557
242.634053	1195.239863	18.519898	-0.046623	2.004992
242.623238	1187.325324	18.524903	-0.046616	1.999418
242.669189	1179.382699	18.529907	-0.046620	1.993814
242.576084	1171.461177	18.534912	-0.046597	1.988195
242.288656	1163.572305	18.539917	-0.046539	1.982563
242.289100	1155.652286	18.544922	-0.046534	1.976923
242.144744	1147.732754	18.549927	-0.046502	1.971252
242.037661	1139.800291	18.554931	-0.046477	1.965560
242.230408	1131.870828	18.559936	-0.046508	1.959885
242.290649	1123.932246	18.564941	-0.046515	1.954172
242.078258	1115.989659	18.569946	-0.046470	1.948411
242.071884	1108.078756	18.574951	-0.046464	1.942677
241.977476	1100.170297	18.579955	-0.046441	1.936919
242.095202	1092.229996	18.584960	-0.046458	1.931144
241.912577	1084.316097	18.589965	-0.046419	1.925338
241.909511	1076.433352	18.594970	-0.046414	1.919557
241.849126	1068.527244	18.599975	-0.046398	1.913734
241.623833	1060.610557	18.604979	-0.046351	1.907868
241.631227	1052.710765	18.609984	-0.046347	1.902022
241.587537	1044.795510	18.614989	-0.046334	1.896141
241.439140	1036.885323	18.619994	-0.046302	1.890234
241.261308	1029.009015	18.624999	-0.046264	1.884330
241.145819	1021.112884	18.630003	-0.046237	1.878399
241.322888	1013.171509	18.635008	-0.046265	1.872450
241.007254	1005.265188	18.640013	-0.046201	1.866451
240.893362	997.377011	18.645018	-0.046175	1.860470
240.881762	989.492267	18.650023	-0.046168	1.854483
240.536350	981.590500	18.655027	-0.046099	1.848426
240.598846	973.673829	18.660032	-0.046106	1.842385
240.608228	965.767591	18.665037	-0.046102	1.836326
240.669932	957.830123	18.670042	-0.046109	1.830229
240.603701	949.939893	18.675047	-0.046092	1.824132
240.180222	942.097045	18.680051	-0.046008	1.818010
240.368486	934.168396	18.685056	-0.046038	1.811873
240.148818	926.268985	18.690061	-0.045992	1.805689
240.109471	918.392433	18.695066	-0.045980	1.799524
240.230852	910.470940	18.700071	-0.045998	1.793321
240.036524	902.539741	18.705075	-0.045957	1.787051
239.919098	894.673280	18.710080	-0.045930	1.780819
239.818970	886.789685	18.715085	-0.045906	1.774554
239.701893	878.905486	18.720090	-0.045879	1.768264
239.623794	871.030654	18.725095	-0.045860	1.761964
239.751463	863.116364	18.730099	-0.045879	1.755636
239.494765	855.257511	18.735104	-0.045826	1.749280
239.524282	847.354510	18.740109	-0.045827	1.742903
239.597587	839.463510	18.745114	-0.045835	1.736516
239.359413	831.611903	18.750119	-0.045786	1.730099
238.922264	823.797342	18.755123	-0.045700	1.723663
239.055368	815.894460	18.760128	-0.045720	1.717203
239.088190	807.975348	18.765133	-0.045721	1.710693
238.988588	800.098650	18.770138	-0.045697	1.704175
238.819766	792.260594	18.775143	-0.045661	1.697656
238.619077	784.387767	18.780147	-0.045619	1.691078
238.483843	776.541524	18.785152	-0.045589	1.684505
238.504643	768.651702	18.790157	-0.045588	1.677890
238.450054	760.773583	18.795162	-0.045573	1.671250
238.778820	752.829859	18.800167	-0.045629	1.664578
238.369907	745.039294	18.805171	-0.045548	1.657911
238.462065	737.151051	18.810176	-0.045560	1.651201
238.430645	729.277789	18.815181	-0.045549	1.644459
238.319354	721.454945	18.820186	-0.045524	1.637723
237.960580	713.598378	18.825191	-0.045452	1.630895
238.110291	705.673845	18.830195	-0.045475	1.624050
238.279477	697.806771	18.835200	-0.045502	1.617228
238.157539	689.956857	18.840205	-0.045474	1.610353
237.874611	682.152134	18.845210	-0.045416	1.603464
237.841389	674.322192	18.850215	-0.045405	1.596559
237.567229	666.482446	18.855219	-0.045349	1.589581
237.590464	658.622847	18.860224	-0.045349	1.582597
237.602414	650.776110	18.865229	-0.045346	1.575592
237.414016	642.939707	18.870234	-0.045306	1.568536
237.441601	635.102095	18.875239	-0.045306	1.561478
237.293850	627.284271	18.880243	-0.045274	1.554380
237.496728	619.386917	18.885248	-0.045307	1.547229
237.165383	611.597653	18.890253	-0.045240	1.540065
237.034454	603.779326	18.895258	-0.045211	1.532870
237.206692	595.908168	18.900263	-0.045238	1.525638
236.895135	588.139429	18.905267	-0.045175	1.518394
236.848184	580.309761	18.910272	-0.045162	1.511098
236.698680	572.491303	18.915277	-0.045129	1.503761
236.749250	564.658557	18.920282	-0.045134	1.496406
236.678352	556.836868	18.925287	-0.045115	1.489006
236.346801	549.061744	18.930291	-0.045049	1.481573
236.295330	541.258700	18.935296	-0.045034	1.474119
236.288255	533.383578	18.940301	-0.045028	1.466565
235.993261	525.628164	18.945306	-0.044968	1.459042
236.077518	517.796543	18.950311	-0.044979	1.451467
236.102180	509.978159	18.955315	-0.044979	1.443855
235.840046	502.235536	18.960320	-0.044925	1.436231
235.723795	494.430016	18.965325	-0.044899	1.428527
235.753816	486.622512	18.970330	-0.044899	1.420804
235.790772	478.839421	18.975335	-0.044901	1.413064
235.631965	471.051550	18.980339	-0.044867	1.405244
235.693856	463.277826	18.985344	-0.044874	1.397432
235.378237	455.524296	18.990349	-0.044810	1.389532
235.245743	447.748651	18.995354	-0.044781	1.381596
235.249373	439.981114	19.000359	-0.044776	1.373645
235.019366	432.221402	19.005363	-0.044729	1.365616
234.930937	424.483463	19.010368	-0.044707	1.357587
234.894461	416.699865	19.015373	-0.044696	1.349471
234.792635	408.949559	19.020378	-0.044672	1.341329
234.594772	401.235057	19.025383	-0.044630	1.333159
234.326040	393.498733	19.030387	-0.044576	1.324902
234.357137	385.757935	19.035392	-0.044576	1.316642
233.921325	377.943115	19.040397	-0.044490	1.308166
233.774594	370.208054	19.045402	-0.044458	1.299774
233.681588	362.490311	19.050407	-0.044436	1.291356
233.607398	354.755937	19.055411	-0.044418	1.282868
233.573105	347.044948	19.060416	-0.044406	1.274356
233.327723	339.344036	19.065421	-0.044356	1.265759
233.362527	331.629468	19.070426	-0.044358	1.257141
233.182724	323.942208	19.075431	-0.044319	1.248453
232.750418	316.308188	19.080435	-0.044234	1.239716
232.685160	308.611919	19.085440	-0.044217	1.230917
232.350954	300.944035	19.090445	-0.044150	1.222035
231.677132	293.353304	19.095450	-0.044020	1.213109
231.299520	285.699128	19.100455	-0.043945	1.204103
230.735063	278.089777	19.105459	-0.043835	1.195043
230.410860	270.423226	19.110464	-0.043770	1.185895
230.176594	262.772414	19.115469	-0.043721	1.176712
230.068351	255.096520	19.120474	-0.043696	1.167453
229.714138	247.493889	19.125479	-0.043626	1.158158
229.044303	239.894140	19.130483	-0.043496	1.148725
228.897428	232.245087	19.135488	-0.043464	1.139263
228.432442	224.651604	19.140493	-0.043373	1.129724
227.789459	217.104661	19.145498	-0.043248	1.120122
227.465732	209.512048	19.150503	-0.043183	1.110450
226.965292	201.943331	19.155507	-0.043085	1.100683
226.826454	194.340977	19.160512	-0.043055	1.090866
226.411992	186.788371	19.165517	-0.042973	1.080963
226.057905	179.232042	19.170522	-0.042902	1.070977
225.706650	171.682427	19.175527	-0.042832	1.060906
224.902215	164.215442	19.180531	-0.042678	1.050744
224.488008	156.702297	19.185536	-0.042596	1.040511
224.220910	149.165476	19.190541	-0.042542	1.030180
223.650552	141.692393	19.195546	-0.042431	1.019758
223.244833	134.209340	19.200551	-0.042351	1.009255
222.764923	126.747924	19.205555	-0.042257	0.998653
222.358489	119.259665	19.210560	-0.042176	0.987918
221.799466	111.826710	19.215565	-0.042067	0.977106
221.475653	104.370856	19.220570	-0.042003	0.966198
221.121649	96.955473	19.225575	-0.041932	0.955218
220.391339	89.597804	19.230579	-0.041791	0.944099
219.946325	82.219037	19.235584	-0.041704	0.932889
219.521928	74.847777	19.240589	-0.041620	0.921560
219.027898	67.498388	19.245594	-0.041524	0.910105
218.644936	60.377572	19.250599	-0.041448	0.898893