Tue Mar 23 10:26:54 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.920351	0.019764	0.000000	0.000011	0.720458

0.757443	0.099301	0.005005	0.000042	0.720557
0.751784	0.095715	0.010010	0.000043	0.720548
0.846779	-0.047200	0.015014	0.000025	0.720300
0.737972	-0.062566	0.020019	0.000045	0.720231
0.760428	-0.067154	0.025024	0.000041	0.720230
0.678441	-0.050651	0.030029	0.000057	0.720234
0.550497	-0.029530	0.035034	0.000080	0.720230
0.729583	-0.056817	0.040038	0.000047	0.720239
0.544768	-0.027155	0.045043	0.000082	0.720233
0.647472	-0.043892	0.050048	0.000063	0.720236
0.633046	-0.039854	0.055053	0.000065	0.720239
0.420886	-0.009086	0.060058	0.000105	0.720225
0.529782	-0.020865	0.065062	0.000085	0.720240
0.688036	-0.054545	0.070067	0.000055	0.720229
0.653577	-0.048246	0.075072	0.000062	0.720229
0.786009	-0.067702	0.080077	0.000037	0.720237
0.911525	-0.094641	0.085082	0.000014	0.720228
0.865423	-0.206874	0.090086	0.000022	0.719991
0.888244	-0.255125	0.095091	0.000018	0.719903
0.869406	-0.247253	0.100096	0.000022	0.719912
0.772744	-0.223742	0.105101	0.000040	0.719925
0.608791	-0.199257	0.110106	0.000070	0.719915
0.527427	-0.181598	0.115110	0.000086	0.719921
0.349014	-0.208187	0.120115	0.000119	0.719806
0.506338	-0.333258	0.125120	0.000090	0.719615
0.652751	-0.357503	0.130125	0.000062	0.719618
0.677028	-0.365384	0.135130	0.000058	0.719611
0.762278	-0.378580	0.140134	0.000042	0.719615
0.622434	-0.406234	0.145139	0.000068	0.719511
0.625346	-0.521575	0.150144	0.000068	0.719285
0.561965	-0.505181	0.155149	0.000080	0.719295
0.575036	-0.515971	0.160154	0.000077	0.719278
0.575325	-0.515859	0.165158	0.000077	0.719278
0.621090	-0.677707	0.170163	0.000069	0.718975
0.712260	-0.696152	0.175168	0.000052	0.718970
0.701605	-0.692629	0.180173	0.000054	0.718973
0.551666	-0.724684	0.185178	0.000082	0.718857
0.526516	-0.820061	0.190182	0.000087	0.718660
0.372860	-0.796648	0.195187	0.000115	0.718652
0.510896	-0.821975	0.200192	0.000090	0.718651
0.621143	-0.964471	0.205197	0.000069	0.718408
0.499738	-0.964777	0.210202	0.000092	0.718365
0.888365	-1.031250	0.215206	0.000020	0.718370
0.884294	-1.169536	0.220211	0.000021	0.718095
0.343047	-1.107982	0.225216	0.000122	0.718026
0.307039	-1.100697	0.230221	0.000128	0.718028
0.200674	-1.223501	0.235226	0.000148	0.717748
0.373648	-1.268906	0.240230	0.000116	0.717719
0.467285	-1.294301	0.245235	0.000099	0.717701
0.339076	-1.427750	0.250240	0.000123	0.717392
0.368069	-1.429160	0.255245	0.000117	0.717399
0.380025	-1.495319	0.260250	0.000115	0.717273
0.460451	-1.596498	0.265254	0.000100	0.717101
0.407121	-1.586878	0.270259	0.000110	0.717101
0.313282	-1.725488	0.275264	0.000128	0.716793
0.232194	-1.721253	0.280269	0.000143	0.716773
0.176941	-1.793006	0.285274	0.000153	0.716611
-0.058828	-1.827310	0.290278	0.000197	0.716460
-0.065139	-1.839303	0.295283	0.000199	0.716434
-0.155613	-1.975451	0.300288	0.000216	0.716132
-0.015513	-1.995396	0.305293	0.000190	0.716142
-0.291463	-2.041118	0.310298	0.000241	0.715954
-0.300950	-2.067381	0.315302	0.000243	0.715899
-0.144856	-2.171281	0.320307	0.000214	0.715748
-0.254341	-2.250258	0.325312	0.000234	0.715552
-0.232194	-2.290088	0.330317	0.000230	0.715481
-1.383129	-2.208711	0.335322	0.000445	0.715236
-2.084575	-2.081882	0.340326	0.000575	0.715239
-2.202198	-2.173609	0.345331	0.000597	0.715016
-3.222518	-2.045425	0.350336	0.000787	0.714909
-3.150932	-2.052549	0.355341	0.000774	0.714920
-3.154698	-2.142254	0.360346	0.000775	0.714741
-4.006427	-2.053860	0.365350	0.000933	0.714615
-4.089358	-2.037905	0.370355	0.000949	0.714617
-4.251996	-2.017616	0.375360	0.000979	0.714600
-4.607732	-2.109485	0.380365	0.001045	0.714292
-5.167670	-2.011785	0.385370	0.001150	0.714288
-5.262842	-1.988386	0.390374	0.001167	0.714300
-4.926971	-2.058971	0.395379	0.001105	0.714279
-5.612403	-2.090899	0.400384	0.001233	0.713973
-5.751256	-2.061293	0.405389	0.001259	0.713982
-5.973258	-2.021743	0.410394	0.001300	0.713982
-5.558968	-2.095457	0.415398	0.001223	0.713982
-6.256799	-2.085309	0.420403	0.001353	0.713755
-7.291825	-1.948110	0.425408	0.001546	0.713661
-6.606267	-2.064966	0.430413	0.001418	0.713672
-6.842023	-2.029049	0.435418	0.001462	0.713659
-6.897870	-2.013445	0.440422	0.001472	0.713671
-7.050365	-2.100110	0.445427	0.001501	0.713444
-7.904200	-1.987120	0.450432	0.001660	0.713366
-7.731275	-2.014154	0.455437	0.001628	0.713374
-7.558114	-2.050644	0.460442	0.001595	0.713362
-7.596991	-2.038772	0.465446	0.001603	0.713372
-7.867728	-2.065575	0.470451	0.001653	0.713223
-8.832196	-1.986112	0.475456	0.001833	0.713039
-8.356981	-2.065586	0.480461	0.001744	0.713049
-8.981733	-1.961739	0.485466	0.001861	0.713034
-9.175880	-1.921150	0.490470	0.001897	0.713046
-8.312292	-2.079768	0.495475	0.001736	0.713036
-8.646727	-2.103144	0.500480	0.001799	0.712871
-9.439095	-2.036574	0.505485	0.001946	0.712723
-9.147836	-2.093472	0.510490	0.001892	0.712712
-9.055659	-2.106831	0.515494	0.001875	0.712718
-9.402013	-2.045322	0.520499	0.001939	0.712718
-9.567377	-2.017191	0.525504	0.001970	0.712715
-9.321549	-2.184214	0.530509	0.001925	0.712470
-10.508992	-2.011961	0.535514	0.002146	0.712391
-10.398583	-2.027630	0.540518	0.002125	0.712399
-10.038540	-2.094665	0.545523	0.002058	0.712393
-10.592573	-1.995295	0.550528	0.002161	0.712395
-10.333732	-2.039483	0.555533	0.002113	0.712398
-10.573318	-2.085589	0.560538	0.002158	0.712221
-11.370224	-1.999769	0.565542	0.002306	0.712109
-11.295995	-2.018078	0.570547	0.002292	0.712099
-11.349704	-2.011834	0.575552	0.002303	0.712092
-11.224210	-2.028822	0.580557	0.002279	0.712103
-11.739544	-1.944409	0.585562	0.002375	0.712088
-11.718525	-1.940162	0.590566	0.002371	0.712104
-11.565189	-2.038299	0.595571	0.002343	0.711963
-12.307740	-2.001433	0.600576	0.002481	0.711772
-11.683447	-2.110772	0.605581	0.002365	0.711776
-12.669206	-1.937144	0.610586	0.002548	0.711772
-12.329085	-1.995542	0.615590	0.002485	0.711776
-12.133914	-2.029995	0.620595	0.002449	0.711777
-12.322938	-2.000033	0.625600	0.002484	0.711769
-12.162279	-2.120022	0.630605	0.002454	0.711587
-12.905733	-2.053250	0.635610	0.002593	0.711456
-13.078994	-2.016940	0.640614	0.002625	0.711467
-13.057221	-2.021323	0.645619	0.002621	0.711466
-13.112875	-2.014141	0.650624	0.002631	0.711460
-13.107606	-2.010068	0.655629	0.002631	0.711470
-13.334172	-1.973728	0.660634	0.002673	0.711462
-13.486224	-2.077459	0.665638	0.002701	0.711201
-14.076933	-1.997315	0.670643	0.002811	0.711151
-14.403024	-1.939096	0.675648	0.002872	0.711151
-13.736369	-2.055675	0.680653	0.002748	0.711155
-14.110312	-1.991550	0.685658	0.002818	0.711150
-14.336814	-1.949079	0.690662	0.002860	0.711154
-14.064490	-1.994621	0.695667	0.002809	0.711160
-14.056793	-2.074416	0.700672	0.002808	0.711003
-14.819198	-1.993457	0.705677	0.002950	0.710894
-15.183643	-1.933640	0.710682	0.003018	0.710883
-14.779445	-2.002797	0.715686	0.002942	0.710889
-14.838811	-1.993935	0.720691	0.002953	0.710885
-15.132569	-1.944445	0.725696	0.003008	0.710880
-14.604170	-2.032917	0.730701	0.002910	0.710891
-14.956019	-2.068549	0.735706	0.002976	0.710694
-16.290607	-1.896750	0.740710	0.003224	0.710562
-15.771076	-1.994467	0.745715	0.003127	0.710552
-15.983826	-1.958822	0.750720	0.003167	0.710548
-15.608422	-2.025469	0.755725	0.003097	0.710548
-15.827273	-1.992722	0.760730	0.003138	0.710535
-15.749974	-2.000317	0.765734	0.003124	0.710548
-15.938117	-2.018939	0.770739	0.003159	0.710443
-16.887258	-1.960343	0.775744	0.003335	0.710222
-16.374097	-2.044040	0.780749	0.003240	0.710238
-16.602496	-2.010681	0.785754	0.003282	0.710223
-17.019037	-1.933569	0.790758	0.003360	0.710229
-16.576567	-2.011933	0.795763	0.003278	0.710230
-16.880050	-1.959104	0.800768	0.003334	0.710227
-16.508812	-2.085724	0.805773	0.003265	0.710106
-17.976699	-1.928044	0.810778	0.003539	0.709898
-17.457691	-2.019423	0.815782	0.003442	0.709900
-17.416138	-2.021865	0.820787	0.003434	0.709910
-17.925277	-1.936568	0.825792	0.003529	0.709899
-17.622976	-1.985548	0.830797	0.003473	0.709909
-17.905943	-1.932627	0.835802	0.003526	0.709914
-17.973396	-1.921579	0.840806	0.003538	0.709912
-18.104760	-2.025690	0.845811	0.003563	0.709657
-18.595827	-1.962100	0.850816	0.003654	0.709609
-18.531464	-1.969623	0.855821	0.003642	0.709617
-18.706610	-1.944262	0.860826	0.003675	0.709605
-18.730268	-1.935517	0.865830	0.003679	0.709614
-18.369292	-2.002250	0.870835	0.003612	0.709609
-18.387157	-2.003042	0.875840	0.003616	0.709601
-18.604787	-2.081311	0.880845	0.003656	0.709366
-19.481062	-1.973558	0.885850	0.003819	0.709270
-19.382536	-1.986937	0.890854	0.003801	0.709278
-19.242283	-2.007479	0.895859	0.003775	0.709287
-19.598634	-1.946199	0.900864	0.003841	0.709282
-19.485004	-1.960359	0.905869	0.003820	0.709294
-19.568155	-1.954545	0.910874	0.003836	0.709276
-19.581604	-2.053859	0.915878	0.003838	0.709072
-20.222544	-1.985873	0.920883	0.003958	0.708980
-20.579998	-1.929578	0.925888	0.004024	0.708965
-20.270766	-1.979999	0.930893	0.003967	0.708974
-20.432821	-1.954001	0.935898	0.003997	0.708968
-20.396251	-1.959578	0.940902	0.003990	0.708970
-20.357303	-1.963473	0.945907	0.003983	0.708976
-20.736582	-1.952509	0.950912	0.004054	0.708863
-21.443434	-1.921266	0.955917	0.004185	0.708673
-21.055362	-2.002179	0.960922	0.004113	0.708649
-21.230835	-1.966737	0.965926	0.004146	0.708657
-21.259668	-1.954972	0.970931	0.004151	0.708671
-21.227927	-1.971063	0.975936	0.004145	0.708650
-21.129624	-1.985108	0.980941	0.004127	0.708656
-21.092134	-2.025363	0.985946	0.004120	0.708589
-21.912697	-1.991068	0.990950	0.004273	0.708365
-21.997539	-1.974465	0.995955	0.004289	0.708368
-22.447192	-1.897486	1.000960	0.004373	0.708361
-22.042250	-1.967772	1.005965	0.004297	0.708365
-22.240943	-1.934347	1.010970	0.004334	0.708361
-22.358726	-1.914171	1.015974	0.004356	0.708359
-21.819747	-2.025748	1.020979	0.004256	0.708328
-22.815722	-2.002223	1.025984	0.004442	0.708019
-22.993828	-1.964835	1.030989	0.004475	0.708030
-23.199343	-1.931243	1.035994	0.004513	0.708024
-23.040160	-1.958748	1.040998	0.004483	0.708026
-22.849639	-1.990593	1.046003	0.004448	0.708030
-23.100559	-1.951673	1.051008	0.004495	0.708018
-22.886898	-1.999473	1.056013	0.004455	0.707999
-23.729559	-1.997821	1.061018	0.004612	0.707701
-24.009454	-1.940274	1.066022	0.004664	0.707716
-23.834087	-1.974360	1.071027	0.004632	0.707710
-24.264999	-1.895035	1.076032	0.004712	0.707715
-24.193625	-1.901681	1.081037	0.004699	0.707727
-23.987754	-1.946727	1.086042	0.004660	0.707710
-23.861890	-1.967363	1.091046	0.004637	0.707714
-23.930021	-2.055414	1.096051	0.004650	0.707513
-25.536874	-1.829521	1.101056	0.004949	0.707391
-24.787906	-1.961435	1.106061	0.004810	0.707394
-24.688571	-1.983098	1.111066	0.004791	0.707386
-25.022730	-1.921443	1.116070	0.004853	0.707390
-24.655290	-1.986531	1.121075	0.004785	0.707391
-24.691312	-1.987572	1.126080	0.004792	0.707376
-24.975657	-1.995485	1.131085	0.004845	0.707258
-25.857108	-1.919090	1.136090	0.005009	0.707096
-25.452814	-1.991486	1.141094	0.004934	0.707096
-25.722848	-1.940520	1.146099	0.004984	0.707101
-25.988201	-1.888911	1.151104	0.005033	0.707110
-25.409956	-1.993162	1.156109	0.004926	0.707107
-25.464322	-1.989065	1.161114	0.004936	0.707096
-26.317940	-1.909138	1.166118	0.005095	0.706951
-26.605581	-1.947465	1.171123	0.005149	0.706771
-26.337215	-1.999989	1.176128	0.005099	0.706761
-26.444293	-1.974801	1.181133	0.005119	0.706773
-26.862803	-1.901376	1.186138	0.005197	0.706771
-26.693501	-1.932748	1.191142	0.005165	0.706768
-26.715424	-1.926466	1.196147	0.005169	0.706773
-26.627250	-1.985449	1.201152	0.005153	0.706686
-26.996712	-2.036767	1.206157	0.005222	0.706451
-27.152766	-2.010387	1.211162	0.005251	0.706448
-27.626763	-1.920313	1.216166	0.005339	0.706459
-27.254300	-1.986029	1.221171	0.005270	0.706460
-27.120687	-2.016322	1.226176	0.005245	0.706447
-27.616398	-1.919194	1.231181	0.005337	0.706464
-27.560670	-2.027037	1.236186	0.005327	0.706268
-28.176633	-1.983664	1.241190	0.005442	0.706134
-27.961857	-2.018833	1.246195	0.005402	0.706140
-28.211439	-1.979236	1.251200	0.005448	0.706130
-27.956378	-2.018519	1.256205	0.005401	0.706143
-27.764705	-2.057759	1.261210	0.005365	0.706132
-28.356664	-1.978681	1.266214	0.005475	0.706079
-28.949745	-1.973935	1.271219	0.005586	0.705876
-28.562454	-2.045168	1.276224	0.005514	0.705871
-28.789896	-2.001794	1.281229	0.005556	0.705877
-29.289458	-1.915002	1.286234	0.005649	0.705872
-29.028254	-1.961707	1.291238	0.005601	0.705872
-28.988643	-1.963020	1.296243	0.005593	0.705883
-29.328054	-1.997056	1.301248	0.005657	0.705693
-29.879491	-1.975204	1.306253	0.005759	0.705539
-29.739002	-1.998417	1.311258	0.005733	0.705543
-29.944367	-1.967703	1.316262	0.005772	0.705531
-29.926242	-1.968291	1.321267	0.005768	0.705536
-29.606423	-2.029865	1.326272	0.005709	0.705527
-29.472531	-2.052793	1.331277	0.005684	0.705529
-30.364634	-2.044978	1.336282	0.005850	0.705224
-30.482346	-2.027170	1.341286	0.005872	0.705218
-30.807301	-1.964169	1.346291	0.005933	0.705228
-31.215908	-1.896412	1.351296	0.006009	0.705217
-30.964324	-1.933225	1.356301	0.005962	0.705234
-30.987997	-1.926714	1.361306	0.005966	0.705238
-30.950542	-1.939974	1.366310	0.005959	0.705225
-30.918603	-2.054014	1.371315	0.005954	0.705006
-31.953271	-1.925495	1.376320	0.006146	0.704894
-31.860822	-1.936118	1.381325	0.006129	0.704905
-31.734295	-1.959053	1.386330	0.006105	0.704905
-31.880385	-1.932388	1.391334	0.006133	0.704906
-31.833866	-1.939087	1.396339	0.006124	0.704909
-31.842593	-1.942833	1.401344	0.006126	0.704898
-31.698503	-2.016352	1.406349	0.006099	0.704802
-32.418890	-1.987668	1.411354	0.006233	0.704601
-32.633045	-1.950111	1.416358	0.006273	0.704599
-32.796460	-1.915556	1.421363	0.006304	0.704610
-32.435315	-1.989643	1.426368	0.006236	0.704590
-32.322171	-2.002797	1.431373	0.006215	0.704604
-32.648005	-1.947811	1.436378	0.006276	0.704598
-32.752014	-2.010729	1.441382	0.006296	0.704434
-33.288882	-1.993297	1.446387	0.006396	0.704276
-33.789728	-1.903591	1.451392	0.006489	0.704277
-33.631412	-1.931418	1.456397	0.006459	0.704277
-33.478956	-1.959905	1.461402	0.006431	0.704275
-33.451922	-1.962783	1.466406	0.006426	0.704279
-33.428937	-1.965211	1.471411	0.006422	0.704282
-33.557965	-2.002232	1.476416	0.006446	0.704161
-34.322036	-1.963726	1.481421	0.006588	0.703964
-34.112771	-2.002764	1.486426	0.006549	0.703960
-34.279500	-1.976482	1.491430	0.006580	0.703953
-34.119693	-1.996104	1.496435	0.006551	0.703971
-34.647180	-1.901724	1.501440	0.006649	0.703971
-34.580846	-1.914588	1.506445	0.006637	0.703969
-34.183548	-2.051125	1.511450	0.006563	0.703836
-35.389581	-1.931466	1.516454	0.006787	0.703644
-35.133873	-1.974143	1.521459	0.006740	0.703650
-35.369018	-1.933498	1.526464	0.006784	0.703647
-34.778768	-2.037471	1.531469	0.006674	0.703650
-34.987814	-2.002136	1.536474	0.006713	0.703646
-35.496391	-1.908689	1.541478	0.006807	0.703651
-35.087313	-2.053134	1.546483	0.006731	0.703507
-36.049339	-1.960147	1.551488	0.006910	0.703348
-35.934994	-1.978631	1.556493	0.006889	0.703352
-36.051742	-1.958394	1.561498	0.006911	0.703351
-35.916195	-1.982474	1.566502	0.006886	0.703351
-35.785990	-2.000887	1.571507	0.006862	0.703360
-36.151649	-1.941303	1.576512	0.006930	0.703349
-36.338778	-2.044852	1.581517	0.006965	0.703072
-36.914010	-1.972244	1.586522	0.007072	0.703012
-36.949351	-1.967599	1.591526	0.007078	0.703008
-36.406315	-2.059145	1.596531	0.006977	0.703019
-37.198260	-1.923758	1.601536	0.007125	0.703007
-37.272559	-1.901043	1.606541	0.007139	0.703026
-37.201626	-1.907888	1.611546	0.007126	0.703038
-37.381179	-1.992988	1.616550	0.007159	0.702801
-38.209396	-1.887430	1.621555	0.007313	0.702716
-38.006160	-1.930027	1.626560	0.007276	0.702703
-37.332692	-2.049038	1.631565	0.007150	0.702705
-38.098377	-1.910681	1.636570	0.007293	0.702708
-38.163854	-1.902826	1.641574	0.007305	0.702701
-37.698131	-1.982794	1.646579	0.007218	0.702707
-38.094155	-1.972345	1.651584	0.007292	0.702585
-38.737247	-1.958674	1.656589	0.007412	0.702381
-38.362695	-2.023358	1.661594	0.007342	0.702385
-39.284163	-1.850009	1.666598	0.007514	0.702403
-39.216841	-1.854325	1.671603	0.007501	0.702419
-39.255078	-1.853100	1.676608	0.007508	0.702407
-39.217725	-1.857901	1.681613	0.007502	0.702411
-38.764438	-1.949434	1.686618	0.007417	0.702389
-39.170824	-1.983757	1.691622	0.007493	0.702173
-39.780551	-1.905146	1.696627	0.007607	0.702112
-39.937087	-1.886917	1.701632	0.007636	0.702092
-39.605800	-1.944583	1.706637	0.007574	0.702095
-39.678236	-1.936834	1.711642	0.007588	0.702085
-39.539496	-1.962913	1.716646	0.007562	0.702082
-39.214954	-2.017179	1.721651	0.007502	0.702089
-40.071857	-2.006653	1.726656	0.007661	0.701801
-40.200702	-2.006890	1.731661	0.007685	0.701754
-40.410249	-1.971416	1.736666	0.007724	0.701750
-40.601727	-1.934459	1.741670	0.007760	0.701756
-40.353530	-1.977739	1.746675	0.007714	0.701758
-40.354249	-1.984353	1.751680	0.007714	0.701744
-40.423388	-2.012891	1.756685	0.007727	0.701661
-41.478878	-1.929058	1.761690	0.007923	0.701450
-41.122232	-1.997724	1.766694	0.007857	0.701439
-41.239887	-1.970846	1.771699	0.007879	0.701451
-41.542703	-1.922442	1.776704	0.007935	0.701440
-41.162207	-1.988231	1.781709	0.007865	0.701444
-41.056226	-2.006542	1.786714	0.007845	0.701445
-41.470714	-2.021234	1.791718	0.007922	0.701265
-41.917453	-2.007385	1.796723	0.008005	0.701132
-42.002186	-1.992966	1.801728	0.008021	0.701131
-42.067717	-1.981894	1.806733	0.008033	0.701129
-41.957837	-2.000747	1.811738	0.008013	0.701131
-41.831200	-2.024437	1.816742	0.007990	0.701128
-42.097262	-1.982466	1.821747	0.008039	0.701117
-42.725761	-1.988764	1.826752	0.008156	0.700877
-42.298030	-2.061707	1.831757	0.008077	0.700884
-42.599465	-2.007420	1.836762	0.008133	0.700885
-42.976520	-1.942229	1.841766	0.008203	0.700881
-42.446898	-2.033686	1.846771	0.008104	0.700887
-42.581662	-2.013966	1.851776	0.008130	0.700878
-43.248936	-2.060961	1.856781	0.008254	0.700541
-43.664348	-1.987466	1.861786	0.008331	0.700540
-44.029816	-1.926071	1.866790	0.008399	0.700532
-43.456769	-2.023696	1.871795	0.008293	0.700541
-43.497766	-2.021616	1.876800	0.008300	0.700531
-43.701250	-1.981096	1.881805	0.008338	0.700539
-43.549563	-2.075101	1.886810	0.008310	0.700403
-45.102120	-1.887464	1.891814	0.008599	0.700222
-44.425891	-2.003683	1.896819	0.008473	0.700231
-44.262497	-2.036658	1.901824	0.008443	0.700223
-44.421072	-2.006763	1.906829	0.008473	0.700226
-44.280147	-2.033193	1.911834	0.008446	0.700224
-44.369365	-2.019203	1.916838	0.008463	0.700220
-44.656443	-2.095749	1.921843	0.008517	0.699960
-45.647598	-1.948781	1.926848	0.008701	0.699900
-45.674095	-1.941090	1.931853	0.008706	0.699906
-45.161910	-2.032025	1.936858	0.008611	0.699907
-45.700862	-1.935576	1.941862	0.008711	0.699907
-45.477916	-1.973208	1.946867	0.008670	0.699911
-45.557703	-1.959130	1.951872	0.008685	0.699911
-45.798626	-2.026432	1.956877	0.008730	0.699687
-46.530034	-1.934757	1.961882	0.008866	0.699608
-46.348965	-1.968959	1.966886	0.008832	0.699604
-45.885271	-2.045753	1.971891	0.008746	0.699616
-46.344074	-1.974125	1.976896	0.008831	0.699595
-46.347325	-1.970504	1.981901	0.008832	0.699602
-46.066390	-2.018977	1.986906	0.008780	0.699605
-46.837959	-2.034409	1.991910	0.008923	0.699294
-47.115042	-1.993140	1.996915	0.008975	0.699277
-47.055593	-2.006518	2.001920	0.008964	0.699271

-47.238987	-1.974767	2.011917	0.008998	0.699269
-47.152214	-1.991229	2.021914	0.008982	0.699267
-46.919517	-2.032750	2.031910	0.008939	0.699267
-47.838586	-2.015223	2.041907	0.009110	0.698969
-47.448031	-2.030907	2.051904	0.009038	0.699079
-47.864009	-1.920688	2.061901	0.009115	0.699152
-47.259105	-1.968693	2.071898	0.009002	0.699273
-46.956202	-2.022424	2.081894	0.008946	0.699274
-47.147060	-1.990189	2.091891	0.008982	0.699270
-46.969129	-2.022521	2.101888	0.008949	0.699269
-47.034096	-2.010387	2.111885	0.008961	0.699269
-47.015529	-2.014457	2.121882	0.008958	0.699268
-46.928331	-2.027033	2.131878	0.008941	0.699274
-47.005684	-2.011729	2.141875	0.008956	0.699276
-47.048061	-1.951960	2.151872	0.008964	0.699382
-46.226037	-1.988476	2.161869	0.008811	0.699606
-46.286719	-1.975105	2.171866	0.008822	0.699611
-46.209596	-1.990732	2.181862	0.008808	0.699607
-46.154719	-2.003893	2.191859	0.008798	0.699600
-45.540663	-1.976031	2.201856	0.008684	0.699878
-45.591683	-1.956105	2.211853	0.008693	0.699900
-45.129499	-2.039851	2.221850	0.008607	0.699897
-45.640013	-1.942037	2.231846	0.008702	0.699911
-44.868535	-1.923035	2.241843	0.008559	0.700228
-44.605483	-1.969503	2.251840	0.008510	0.700229
-44.787314	-1.938343	2.261837	0.008544	0.700226
-44.334444	-1.950660	2.271834	0.008460	0.700365
-43.669250	-1.984362	2.281830	0.008336	0.700537
-43.699770	-1.977446	2.291827	0.008342	0.700540
-43.932188	-1.937152	2.301824	0.008385	0.700537
-42.913927	-1.966739	2.311821	0.008196	0.700845
-42.592360	-2.007405	2.321818	0.008136	0.700879
-42.718676	-1.984257	2.331814	0.008159	0.700880
-42.739753	-1.977095	2.341811	0.008163	0.700887
-42.320042	-1.932440	2.351808	0.008085	0.701129
-42.081714	-1.975191	2.361805	0.008041	0.701128
-42.131617	-1.963159	2.371802	0.008051	0.701134
-41.853346	-1.896984	2.381798	0.007999	0.701368
-41.301941	-1.960089	2.391795	0.007896	0.701440
-41.189619	-1.978290	2.401792	0.007875	0.701443
-40.951358	-1.954955	2.411789	0.007831	0.701576
-40.286673	-1.987438	2.421786	0.007707	0.701750
-40.419456	-1.964141	2.431782	0.007732	0.701749
-40.229422	-1.998203	2.441779	0.007697	0.701749
-39.761967	-1.926174	2.451776	0.007610	0.702063
-39.502350	-1.965649	2.461773	0.007562	0.702077
-39.534036	-1.955161	2.471770	0.007568	0.702086
-39.103295	-1.954485	2.481766	0.007488	0.702243
-38.772291	-1.943545	2.491763	0.007426	0.702384
-38.933422	-1.916045	2.501760	0.007456	0.702381
-38.691044	-1.906568	2.511757	0.007411	0.702488
-37.701439	-1.976244	2.521754	0.007227	0.702703
-37.986044	-1.926155	2.531750	0.007280	0.702702
-37.732161	-1.972448	2.541747	0.007233	0.702700
-37.225343	-1.919937	2.551744	0.007139	0.702988
-36.973491	-1.947919	2.561741	0.007092	0.703022
-37.092506	-1.927273	2.571738	0.007114	0.703021
-36.720315	-1.901344	2.581734	0.007045	0.703207
-36.080801	-1.942857	2.591731	0.006926	0.703353
-35.980206	-1.961360	2.601728	0.006907	0.703352
-36.147235	-1.922016	2.611725	0.006938	0.703371
-35.338223	-1.928182	2.621722	0.006788	0.703650
-35.442933	-1.906254	2.631718	0.006807	0.703656
-35.253927	-1.939781	2.641715	0.006772	0.703656
-34.932915	-1.886242	2.651712	0.006713	0.703879
-34.222303	-1.974634	2.661709	0.006580	0.703957
-34.464482	-1.928820	2.671706	0.006626	0.703962
-34.242882	-1.932711	2.681702	0.006584	0.704033
-33.539560	-1.939273	2.691699	0.006454	0.704273
-33.677932	-1.914598	2.701696	0.006479	0.704273
-33.501134	-1.948001	2.711693	0.006447	0.704269
-32.768257	-1.941953	2.721690	0.006310	0.704544
-32.437639	-1.971486	2.731686	0.006249	0.704603
-32.346545	-1.992327	2.741683	0.006232	0.704594
-32.560174	-1.948656	2.751680	0.006272	0.704605
-31.680656	-1.962429	2.761677	0.006108	0.704893
-31.634884	-1.970539	2.771674	0.006100	0.704893
-31.496093	-1.996315	2.781670	0.006074	0.704890
-31.540690	-1.916821	2.791667	0.006082	0.705034
-30.781834	-1.962396	2.801664	0.005941	0.705215
-30.690980	-1.981180	2.811661	0.005924	0.705209
-30.693522	-1.981222	2.821658	0.005925	0.705208
-29.704444	-2.023045	2.831654	0.005741	0.705479
-29.990679	-1.948413	2.841651	0.005794	0.705526
-29.784056	-1.986239	2.851648	0.005756	0.705524
-29.561061	-2.012153	2.861645	0.005714	0.705552
-28.974867	-1.960654	2.871642	0.005605	0.705865
-28.618906	-2.024825	2.881638	0.005539	0.705864
-29.021242	-1.952485	2.891635	0.005614	0.705865
-28.715551	-1.952221	2.901632	0.005557	0.705975
-28.008239	-2.002660	2.911629	0.005426	0.706127
-28.130980	-1.978870	2.921626	0.005449	0.706130
-27.945101	-2.011600	2.931622	0.005414	0.706131
-27.481716	-1.939398	2.941619	0.005328	0.706442
-27.339568	-1.963206	2.951616	0.005302	0.706445
-27.285382	-1.972115	2.961613	0.005292	0.706446
-26.872941	-1.944200	2.971610	0.005215	0.706650
-26.447625	-1.967405	2.981606	0.005136	0.706755
-26.615342	-1.933071	2.991603	0.005167	0.706764
-26.273988	-1.945817	3.001600	0.005104	0.706861
-25.560173	-1.959055	3.011597	0.004971	0.707089
-25.611557	-1.949227	3.021594	0.004980	0.707090
-25.541526	-1.962048	3.031590	0.004967	0.707090
-25.044221	-1.910149	3.041587	0.004875	0.707372
-24.745261	-1.959485	3.051584	0.004819	0.707379
-24.711849	-1.965157	3.061581	0.004813	0.707380
-24.366560	-1.934749	3.071578	0.004749	0.707564
-23.673440	-1.988971	3.081574	0.004620	0.707703
-23.834128	-1.962468	3.091571	0.004650	0.707698
-23.687315	-1.981260	3.101568	0.004623	0.707713
-22.966911	-1.962048	3.111565	0.004489	0.708009
-22.825851	-1.985188	3.121562	0.004463	0.708013
-23.089073	-1.936323	3.131558	0.004512	0.708017
-22.528055	-1.937369	3.141555	0.004407	0.708215
-21.933919	-1.974271	3.151552	0.004297	0.708353
-22.103940	-1.944743	3.161549	0.004329	0.708351
-21.676165	-2.019403	3.171546	0.004249	0.708354
-21.208997	-1.976762	3.181542	0.004162	0.708606
-21.197057	-1.960509	3.191539	0.004160	0.708643
-21.003268	-1.996553	3.201536	0.004124	0.708640
-21.030309	-1.951117	3.211533	0.004129	0.708721
-20.039002	-2.008555	3.221530	0.003945	0.708959
-20.159317	-1.985623	3.231526	0.003967	0.708962
-20.266574	-1.964862	3.241523	0.003987	0.708965
-19.556659	-1.977461	3.251520	0.003855	0.709193
-19.418874	-1.963432	3.261517	0.003830	0.709270
-19.201015	-2.002945	3.271514	0.003789	0.709269
-19.156439	-1.990381	3.281510	0.003781	0.709310
-18.306495	-1.995723	3.291507	0.003623	0.709602
-18.132254	-2.026409	3.301504	0.003590	0.709602
-18.287753	-1.998614	3.311501	0.003619	0.709602
-18.235456	-1.957569	3.321498	0.003610	0.709703
-17.249436	-2.035686	3.331494	0.003426	0.709898
-17.233658	-2.039347	3.341491	0.003423	0.709896
-17.464337	-2.000385	3.351488	0.003466	0.709892
-16.986032	-1.975304	3.361485	0.003377	0.710112
-16.345138	-2.034404	3.371482	0.003258	0.710222
-16.561707	-1.993774	3.381478	0.003299	0.710226
-16.316762	-2.037290	3.391475	0.003253	0.710226
-15.817904	-1.971930	3.401472	0.003160	0.710534
-15.508291	-2.026890	3.411469	0.003103	0.710534
-15.568480	-2.014826	3.421466	0.003114	0.710537
-15.286576	-1.991500	3.431462	0.003062	0.710684
-14.642247	-2.009171	3.441459	0.002942	0.710877
-14.674452	-2.005107	3.451456	0.002948	0.710874
-14.461905	-2.041675	3.461453	0.002908	0.710876
-13.844981	-2.065003	3.471450	0.002794	0.711049
-13.994899	-1.987745	3.481446	0.002822	0.711150
-13.746944	-2.032225	3.491443	0.002776	0.711149
-13.850677	-1.994315	3.501440	0.002795	0.711187
-13.095464	-1.991912	3.511437	0.002654	0.711461
-12.775050	-2.047578	3.521434	0.002595	0.711463
-13.048330	-1.998293	3.531430	0.002646	0.711464
-12.236003	-2.039038	3.541427	0.002495	0.711672
-12.088752	-2.017145	3.551424	0.002467	0.711767
-12.098350	-2.015112	3.561421	0.002469	0.711768
-11.750605	-2.071648	3.571418	0.002405	0.711778
-11.216781	-2.006234	3.581414	0.002305	0.712098
-10.817837	-2.077454	3.591411	0.002231	0.712098
-11.037887	-2.038243	3.601408	0.002272	0.712098
-11.073567	-1.988827	3.611405	0.002279	0.712183
-10.193408	-2.038008	3.621402	0.002115	0.712398
-10.442378	-1.991763	3.631398	0.002162	0.712401
-10.026211	-2.065383	3.641395	0.002084	0.712402
-9.863600	-1.945460	3.651392	0.002054	0.712699
-9.376231	-2.015085	3.661389	0.001963	0.712733
-9.626806	-1.972675	3.671386	0.002010	0.712728
-9.102929	-1.962181	3.681382	0.001913	0.712935
-8.699481	-1.975079	3.691379	0.001838	0.713052
-8.876336	-1.942466	3.701376	0.001871	0.713054
-8.386682	-1.978249	3.711373	0.001779	0.713156
-7.576871	-2.010845	3.721370	0.001629	0.713378
-7.416841	-2.039815	3.731366	0.001599	0.713377
-7.629932	-2.000158	3.741363	0.001639	0.713380
-7.270995	-1.960965	3.751360	0.001572	0.713585
-6.894031	-1.982721	3.761357	0.001502	0.713675
-6.754479	-2.010086	3.771354	0.001476	0.713670
-6.664725	-1.993408	3.781350	0.001459	0.713735
-5.937342	-1.997972	3.791347	0.001324	0.713983
-6.155804	-1.955589	3.801344	0.001365	0.713990
-5.909358	-1.999322	3.811341	0.001319	0.713990
-5.278066	-1.992109	3.821338	0.001202	0.714228
-4.920408	-2.020686	3.831334	0.001135	0.714297
-4.979422	-2.012643	3.841331	0.001146	0.714292
-5.114860	-1.956846	3.851328	0.001172	0.714355
-4.065382	-2.005008	3.861325	0.000976	0.714631
-4.300714	-1.962845	3.871322	0.001020	0.714631
-4.232861	-1.972719	3.881318	0.001008	0.714635
-3.662622	-1.960378	3.891315	0.000901	0.714861
-3.081393	-2.035788	3.901312	0.000793	0.714917
-3.311382	-1.992019	3.911309	0.000836	0.714922
-3.344140	-1.953145	3.921306	0.000842	0.714988
-2.832668	-1.912040	3.931302	0.000747	0.715250
-2.503747	-1.971325	3.941299	0.000686	0.715248
-2.491369	-1.974939	3.951296	0.000684	0.715245
-1.850876	-1.938243	3.961293	0.000565	0.715544
-1.687146	-1.960145	3.971290	0.000534	0.715558
-1.712532	-1.955063	3.981286	0.000539	0.715559
-1.682998	-1.852802	3.991283	0.000534	0.715772
-1.722454	-1.783128	4.001280	0.000541	0.715896
-1.601510	-1.805015	4.011277	0.000519	0.715895
-1.357943	-1.726586	4.021274	0.000473	0.716137
-1.082774	-1.774047	4.031270	0.000422	0.716140
-0.882096	-1.729476	4.041267	0.000385	0.716299
-0.665394	-1.689949	4.051264	0.000345	0.716453
-0.702846	-1.664884	4.061261	0.000352	0.716489
-0.572382	-1.551129	4.071258	0.000327	0.716761
-0.506712	-1.557171	4.081254	0.000315	0.716772
-0.668128	-1.366226	4.091251	0.000345	0.717092
-0.563802	-1.356560	4.101248	0.000326	0.717148
-0.646683	-1.216813	4.111245	0.000341	0.717395
-0.384944	-1.178743	4.121242	0.000293	0.717563
-0.525458	-1.074591	4.131238	0.000319	0.717719
-0.274857	-0.970525	4.141235	0.000272	0.718013
-0.109457	-0.920049	4.151232	0.000242	0.718170
-0.168985	-0.810709	4.161229	0.000253	0.718365
-0.211624	-0.658999	4.171226	0.000261	0.718650
-0.139058	-0.567891	4.181222	0.000247	0.718855
-0.006148	-0.474826	4.191219	0.000222	0.719085
0.036099	-0.362806	4.201216	0.000215	0.719321
0.120515	-0.229366	4.211213	0.000199	0.719614
0.159470	-0.097761	4.221210	0.000192	0.719887
0.143849	0.042662	4.231206	0.000195	0.720158
-0.002338	0.216898	4.241203	0.000222	0.720450
0.000000	0.386578	4.251200	0.000221	0.720784

0.163961	0.982110	4.256205	0.000190	0.722013
0.553808	2.174282	4.261210	0.000117	0.724488
0.525963	4.024147	4.266214	0.000121	0.728093
1.059338	6.337213	4.271219	0.000020	0.732771
1.252840	9.216052	4.276224	-0.000018	0.738391
1.616588	12.538308	4.281229	-0.000087	0.744871
2.079434	16.306246	4.286234	-0.000176	0.752170
2.566379	20.472137	4.291238	-0.000269	0.760150
3.126810	25.033696	4.296243	-0.000377	0.768802
3.290050	30.025889	4.301248	-0.000410	0.778014
3.792829	35.305826	4.306253	-0.000507	0.787745
4.386252	40.896090	4.311258	-0.000621	0.797938
4.848566	46.797829	4.316262	-0.000711	0.808508
5.387560	52.981937	4.321267	-0.000816	0.819454
5.925982	59.429307	4.326272	-0.000920	0.830705
6.472629	66.114149	4.331277	-0.001026	0.842207
8.221371	72.810671	4.336282	-0.001356	0.853926
9.429227	79.831387	4.341286	-0.001585	0.865861
10.723499	87.039110	4.346291	-0.001831	0.877960
11.268429	94.550322	4.351296	-0.001937	0.890167
12.187911	102.157492	4.356301	-0.002113	0.902463
12.909142	109.950545	4.361306	-0.002253	0.914827
13.619953	117.848071	4.366310	-0.002390	0.927183
14.757867	125.806038	4.371315	-0.002607	0.939580
15.564086	133.928364	4.376320	-0.002763	0.951974
16.548993	142.105945	4.381325	-0.002951	0.964335
17.310494	150.417221	4.386330	-0.003098	0.976677
18.298032	158.758209	4.391334	-0.003288	0.988963
19.564770	167.130655	4.396339	-0.003529	1.001211
20.391818	175.606207	4.401344	-0.003689	1.013348
21.077868	184.153160	4.406349	-0.003822	1.025405
21.778618	192.736718	4.411354	-0.003958	1.037376
22.464894	201.321226	4.416358	-0.004091	1.049207
23.423437	209.904599	4.421363	-0.004275	1.060968
24.239429	218.526167	4.426368	-0.004433	1.072617
24.993716	227.163007	4.431373	-0.004579	1.084146
25.624980	235.831224	4.436378	-0.004702	1.095567
26.287329	244.488147	4.441382	-0.004831	1.106862
26.709694	253.214523	4.446387	-0.004915	1.118078
27.771885	261.789326	4.451392	-0.005118	1.129131
28.571923	270.435665	4.456397	-0.005273	1.140108
29.465813	279.077660	4.461402	-0.005445	1.150995
30.559208	287.644256	4.466406	-0.005654	1.161729
31.130693	296.308121	4.471411	-0.005766	1.172374
31.615355	304.957568	4.476416	-0.005862	1.182888
32.591291	313.533476	4.481421	-0.006049	1.193321
33.218854	322.148564	4.486426	-0.006172	1.203639
33.877915	330.740788	4.491430	-0.006300	1.213849
35.050734	339.248506	4.496435	-0.006524	1.223977
35.550091	347.868670	4.501440	-0.006622	1.234019
35.962501	356.458271	4.506445	-0.006705	1.243928
36.786500	364.970298	4.511450	-0.006864	1.253749
37.450149	373.486878	4.516454	-0.006993	1.263469
38.378837	381.969549	4.521459	-0.007171	1.273126
38.681387	390.520176	4.526464	-0.007233	1.282668
39.469950	398.985344	4.531469	-0.007385	1.292136
40.263705	407.437753	4.536474	-0.007539	1.301521
40.645829	416.015283	4.541478	-0.007615	1.310899
41.459538	424.494758	4.546483	-0.007772	1.320184
41.953365	432.925552	4.551488	-0.007870	1.329293
42.455049	441.361030	4.556493	-0.007968	1.338347
42.948518	449.774323	4.561498	-0.008066	1.347315
43.528274	458.170890	4.566502	-0.008179	1.356222
44.163737	466.542530	4.571507	-0.008303	1.365053
44.757027	474.922469	4.576512	-0.008419	1.373829
45.329308	483.296388	4.581517	-0.008531	1.382539
45.724038	491.712627	4.586522	-0.008610	1.391207
46.009698	500.101925	4.591526	-0.008668	1.399776
46.852889	508.401094	4.596531	-0.008831	1.408295
47.235884	516.770159	4.601536	-0.008907	1.416756
47.870326	525.085134	4.606541	-0.009031	1.425154
48.268539	533.444098	4.611546	-0.009110	1.433508
48.848150	541.729542	4.616550	-0.009224	1.441770
49.797277	549.976430	4.621555	-0.009406	1.450007
50.406742	558.280326	4.626560	-0.009525	1.458198
50.616712	566.634863	4.631565	-0.009569	1.466328
51.125672	574.991694	4.636570	-0.009669	1.474463
51.291103	583.304533	4.641574	-0.009705	1.482457
51.896302	591.566362	4.646579	-0.009823	1.490429
52.384838	599.836875	4.651584	-0.009920	1.498347
53.197333	608.046427	4.656589	-0.010076	1.506216
53.818803	616.322454	4.661594	-0.010197	1.514077
54.223759	624.584023	4.666598	-0.010278	1.521851
54.542761	632.887550	4.671603	-0.010343	1.529612
55.053859	641.130405	4.676608	-0.010443	1.537305
55.574448	649.360783	4.681613	-0.010546	1.544950
56.476906	657.571172	4.686618	-0.010719	1.552596
57.239085	665.760785	4.691622	-0.010866	1.560164
57.527007	674.037133	4.696627	-0.010925	1.567705
58.131653	682.261890	4.701632	-0.011043	1.575209
58.551907	690.521115	4.706637	-0.011127	1.582681
58.863295	698.780852	4.711642	-0.011190	1.590103
59.581332	706.965358	4.716646	-0.011329	1.597481
60.274939	715.157148	4.721651	-0.011463	1.604829
60.573344	723.415304	4.726656	-0.011524	1.612145
61.314421	731.600212	4.731661	-0.011668	1.619426
62.028403	739.783806	4.736666	-0.011806	1.626669
62.175728	748.101298	4.741670	-0.011839	1.633918
62.516503	756.317520	4.746675	-0.011907	1.641073
63.002174	764.493208	4.751680	-0.012003	1.648183
63.481595	772.683887	4.756685	-0.012098	1.655273
63.954793	780.869668	4.761690	-0.012191	1.662329
64.297958	789.068185	4.766694	-0.012260	1.669347
64.972819	797.237812	4.771699	-0.012391	1.676356
65.166662	805.444121	4.776704	-0.012433	1.683303
65.699333	813.614467	4.781709	-0.012537	1.690235
66.292966	821.796254	4.786714	-0.012653	1.697157
66.598781	829.987619	4.791718	-0.012715	1.704020
67.567586	838.107263	4.796723	-0.012901	1.710883
67.955248	846.303077	4.801728	-0.012978	1.717706
68.425318	854.449998	4.806733	-0.013071	1.724472
68.986320	862.618040	4.811738	-0.013181	1.731240
69.144349	870.832159	4.816742	-0.013216	1.737968
69.701471	878.987818	4.821747	-0.013325	1.744673
70.066136	887.167299	4.826752	-0.013398	1.751348
70.383886	895.358000	4.831757	-0.013462	1.758000
70.826494	903.500921	4.836762	-0.013550	1.764604
71.265764	911.652893	4.841766	-0.013637	1.771190
71.650390	919.829081	4.846771	-0.013714	1.777764
72.165102	927.958926	4.851776	-0.013815	1.784292
72.912060	936.108349	4.856781	-0.013959	1.790841
73.336899	944.313069	4.861786	-0.014044	1.797370
73.910713	952.396805	4.866790	-0.014156	1.803799
74.463353	960.538167	4.871795	-0.014264	1.810247
74.526526	968.742543	4.876800	-0.014281	1.816662
74.878555	976.873660	4.881805	-0.014352	1.823032
75.492077	984.989935	4.886810	-0.014471	1.829399
75.938343	993.132053	4.891814	-0.014560	1.835745
76.331214	1001.272810	4.896819	-0.014638	1.842061
76.870280	1009.390983	4.901824	-0.014744	1.848355
77.099596	1017.561647	4.906829	-0.014792	1.854631
77.401456	1025.713251	4.911834	-0.014853	1.860880
77.718143	1033.852019	4.916838	-0.014917	1.867100
78.410709	1041.984088	4.921843	-0.015051	1.873338
78.785579	1050.101320	4.926848	-0.015127	1.879507
78.981031	1058.244591	4.931853	-0.015168	1.885655
79.720320	1066.347099	4.936858	-0.015311	1.891814
79.883271	1074.494617	4.941862	-0.015347	1.897921
80.157833	1082.632972	4.946867	-0.015403	1.904015
80.596404	1090.750759	4.951872	-0.015490	1.910092
81.133355	1098.849749	4.956877	-0.015595	1.916146
81.496718	1106.978358	4.961882	-0.015668	1.922184
81.767571	1115.107902	4.966886	-0.015724	1.928194
81.991874	1123.273695	4.971891	-0.015771	1.934206
82.471200	1131.360288	4.976896	-0.015865	1.940169
82.897232	1139.461742	4.981901	-0.015950	1.946119
83.499004	1147.605954	4.986906	-0.016067	1.952101
83.614647	1155.753656	4.991910	-0.016094	1.958015
83.976131	1163.848241	4.996915	-0.016167	1.963898
84.337456	1171.952687	5.001920	-0.016239	1.969771
85.054104	1180.024997	5.006925	-0.016378	1.975642
85.416105	1188.143918	5.011930	-0.016450	1.981490
85.693816	1196.247314	5.016934	-0.016507	1.987302
86.216427	1204.365801	5.021939	-0.016610	1.993132
86.593336	1212.458490	5.026944	-0.016685	1.998912
87.047626	1220.534747	5.031949	-0.016775	2.004672
87.558419	1228.641125	5.036954	-0.016875	2.010442
87.968053	1236.751489	5.041958	-0.016957	2.016188
88.600749	1244.831058	5.046963	-0.017080	2.021918
89.069812	1252.926880	5.051968	-0.017172	2.027627
89.727281	1261.052523	5.056973	-0.017300	2.033360
90.143433	1269.168061	5.061978	-0.017383	2.039045
90.564950	1277.240434	5.066982	-0.017467	2.044684
90.891786	1285.372603	5.071987	-0.017533	2.050340
91.203075	1293.496909	5.076992	-0.017596	2.055973
91.370323	1301.621833	5.081997	-0.017632	2.061577
91.408027	1309.759871	5.087002	-0.017645	2.067161
91.836458	1317.840432	5.092006	-0.017730	2.072730
92.221522	1325.943888	5.097011	-0.017807	2.078295
92.534505	1334.009080	5.102016	-0.017870	2.083812
93.141118	1342.070600	5.107021	-0.017988	2.089341
93.572570	1350.180492	5.112026	-0.018074	2.094870
93.784876	1358.274610	5.117030	-0.018118	2.100353
94.108358	1366.377020	5.122035	-0.018184	2.105838
94.567998	1374.498645	5.127040	-0.018275	2.111335
94.757492	1382.648741	5.132045	-0.018315	2.116810
95.373004	1390.667775	5.137050	-0.018435	2.122224
95.885258	1398.716040	5.142054	-0.018536	2.127634
96.152466	1406.846697	5.147059	-0.018591	2.133062
96.376070	1414.942504	5.152064	-0.018638	2.138449
96.924208	1422.979855	5.157069	-0.018745	2.143814
97.590447	1431.066170	5.162074	-0.018874	2.149208
97.763822	1439.203478	5.167078	-0.018912	2.154577
98.239571	1447.260265	5.172083	-0.019005	2.159907
98.601925	1455.338413	5.177088	-0.019078	2.165228
99.115413	1463.395139	5.182093	-0.019179	2.170536
99.348035	1471.532467	5.187098	-0.019228	2.175857
99.553053	1479.616831	5.192102	-0.019271	2.181128
99.778949	1487.716519	5.197107	-0.019318	2.186398
100.158037	1495.808004	5.202112	-0.019394	2.191664
100.538556	1503.901839	5.207117	-0.019470	2.196919
100.898521	1511.968449	5.212122	-0.019542	2.202142
101.264425	1520.007151	5.217126	-0.019616	2.207335
101.800173	1528.083179	5.222131	-0.019721	2.212555
102.259154	1536.146156	5.227136	-0.019811	2.217747
102.565662	1544.230855	5.232141	-0.019874	2.222927
102.942628	1552.327743	5.237146	-0.019949	2.228110
103.273396	1560.425587	5.242150	-0.020016	2.233276
103.751560	1568.496197	5.247155	-0.020110	2.238427
104.067053	1576.551490	5.252160	-0.020174	2.243541
104.390435	1584.624553	5.257165	-0.020239	2.248656
104.769844	1592.751222	5.262170	-0.020315	2.253797
105.142627	1600.794988	5.267174	-0.020390	2.258874
105.575738	1608.865257	5.272179	-0.020476	2.263962
106.012547	1616.937718	5.277184	-0.020562	2.269039
106.156093	1625.126283	5.282189	-0.020594	2.274153
106.313342	1633.200003	5.287194	-0.020629	2.279184
106.646884	1641.210966	5.292198	-0.020696	2.284181
107.032139	1649.265433	5.297203	-0.020773	2.289198
107.239311	1657.379768	5.302208	-0.020817	2.294225
107.563523	1665.416112	5.307213	-0.020883	2.299204
107.787100	1673.502701	5.312218	-0.020929	2.304194
107.737814	1681.606591	5.317222	-0.020925	2.309161
108.330942	1689.645820	5.322227	-0.021041	2.314131
108.852233	1697.668029	5.327232	-0.021143	2.319075
109.104967	1705.738643	5.332237	-0.021196	2.324014
109.431988	1713.831161	5.337242	-0.021262	2.328963
110.105502	1721.858049	5.342246	-0.021392	2.333890
110.516643	1729.938189	5.347251	-0.021474	2.338817
110.947685	1738.000644	5.352256	-0.021560	2.343724
111.082790	1746.083759	5.357261	-0.021590	2.348610
111.901001	1754.139408	5.362266	-0.021747	2.353524
111.910055	1762.248109	5.367270	-0.021754	2.358394
112.394143	1770.272911	5.372275	-0.021850	2.363242
112.641713	1778.361197	5.377280	-0.021901	2.368099
112.793046	1786.448544	5.382285	-0.021934	2.372938
113.240866	1794.509648	5.387290	-0.022023	2.377775
113.499587	1802.555460	5.392294	-0.022076	2.382578
113.709537	1810.639745	5.397299	-0.022121	2.387390
113.707647	1818.776398	5.402304	-0.022126	2.392207
114.008857	1826.812398	5.407309	-0.022187	2.396978
114.459195	1834.848502	5.412314	-0.022276	2.401752
114.667109	1842.894849	5.417318	-0.022320	2.406503
115.396773	1850.925592	5.422323	-0.022461	2.411276
115.631686	1859.029433	5.427328	-0.022510	2.416044
116.069872	1867.069957	5.432333	-0.022597	2.420781
116.208151	1875.155670	5.437338	-0.022628	2.425512
116.262718	1883.260526	5.442342	-0.022643	2.430238
116.535034	1891.398771	5.447347	-0.022699	2.434992
117.033520	1899.353786	5.452352	-0.022797	2.439647
117.245227	1907.409420	5.457357	-0.022842	2.444329
117.655628	1915.461377	5.462362	-0.022923	2.449016
117.955562	1923.521549	5.467366	-0.022984	2.453690
118.515012	1931.534374	5.472371	-0.023094	2.458347
118.630894	1939.634194	5.477376	-0.023120	2.463012
119.207257	1947.642661	5.482381	-0.023233	2.467650
119.554899	1955.747602	5.487386	-0.023303	2.472317
119.611575	1963.835609	5.492390	-0.023319	2.476944
120.154452	1971.875224	5.497395	-0.023425	2.481571
120.217131	1979.951187	5.502400	-0.023442	2.486175
120.230291	1988.039495	5.507405	-0.023449	2.490773
120.620565	1996.104856	5.512410	-0.023527	2.495378
120.913078	2004.121815	5.517414	-0.023587	2.499939
121.336176	2012.142896	5.522419	-0.023671	2.504504
121.675978	2020.223366	5.527424	-0.023739	2.509088
122.139754	2028.302942	5.532429	-0.023831	2.513672
122.460757	2036.376381	5.537434	-0.023896	2.518234
122.792335	2044.377562	5.542438	-0.023963	2.522747
123.144296	2052.423600	5.547443	-0.024034	2.527279
123.328821	2060.514870	5.552448	-0.024073	2.531816
123.586233	2068.575672	5.557453	-0.024126	2.536334
123.922859	2076.639269	5.562458	-0.024194	2.540850
124.271217	2084.651609	5.567462	-0.024264	2.545330
124.468867	2092.728336	5.572467	-0.024306	2.549828
124.571928	2100.823804	5.577472	-0.024331	2.554322
124.922892	2108.825200	5.582477	-0.024401	2.558773
125.345388	2116.853519	5.587482	-0.024485	2.563235
125.547822	2124.906791	5.592486	-0.024528	2.567689
125.894947	2132.998299	5.597491	-0.024598	2.572166
126.157200	2141.060738	5.602496	-0.024652	2.576613
126.378169	2149.106836	5.607501	-0.024698	2.581041
127.228969	2157.082698	5.612506	-0.024862	2.585465
127.675351	2165.146694	5.617510	-0.024950	2.589903
127.971581	2173.419072	5.622515	-0.025011	2.594436
128.445626	2181.401404	5.627520	-0.025104	2.598815
128.589478	2189.421863	5.632525	-0.025136	2.603186
128.685484	2197.478240	5.637530	-0.025159	2.607565
128.699344	2205.531302	5.642534	-0.025167	2.611929
129.184982	2213.547295	5.647539	-0.025263	2.616298
129.517815	2221.575318	5.652544	-0.025330	2.620656
129.683962	2229.603269	5.657549	-0.025366	2.624995
130.195908	2237.636585	5.662554	-0.025466	2.629353
130.213931	2245.727676	5.667558	-0.025475	2.633702
130.541523	2253.763596	5.672563	-0.025541	2.638034
131.032609	2261.768983	5.677568	-0.025638	2.642354
131.290514	2269.819797	5.682573	-0.025691	2.646676
131.785020	2277.869380	5.687578	-0.025788	2.651005
132.016423	2285.935773	5.692582	-0.025837	2.655319
132.105378	2294.008105	5.697587	-0.025858	2.659620
132.377877	2302.054791	5.702592	-0.025914	2.663912
132.604471	2310.091915	5.707597	-0.025962	2.668189
132.875403	2318.196895	5.712602	-0.026017	2.672498
133.223847	2326.225962	5.717606	-0.026087	2.676765
133.376509	2334.266827	5.722611	-0.026121	2.681019
133.879314	2342.277169	5.727616	-0.026220	2.685272
134.013732	2350.316933	5.732621	-0.026250	2.689510
134.618304	2358.390902	5.737626	-0.026368	2.693790
134.828991	2366.432974	5.742630	-0.026412	2.698021
135.215540	2374.473306	5.747635	-0.026489	2.702255
135.550909	2382.510488	5.752640	-0.026557	2.706478
135.505955	2390.600431	5.757645	-0.026554	2.710698
135.798734	2398.665119	5.762650	-0.026614	2.714919
136.082042	2406.666207	5.767654	-0.026672	2.719100
136.560213	2414.682498	5.772659	-0.026766	2.723294
136.850394	2422.725891	5.777664	-0.026825	2.727485
137.175401	2430.770467	5.782669	-0.026891	2.731671
137.639036	2438.830533	5.787674	-0.026982	2.735868
137.688719	2446.880683	5.792678	-0.026997	2.740028
137.866223	2454.931080	5.797683	-0.027035	2.744189
138.183300	2462.984678	5.802688	-0.027099	2.748354
138.181585	2471.105123	5.807693	-0.027104	2.752528
138.650858	2479.155924	5.812698	-0.027197	2.756688
138.967746	2487.143706	5.817702	-0.027261	2.760800
139.105288	2495.174300	5.822707	-0.027292	2.764918
139.383299	2503.232983	5.827712	-0.027349	2.769051
139.717299	2511.279597	5.832717	-0.027416	2.773176
140.047057	2519.329069	5.837722	-0.027483	2.777296
140.255556	2527.348856	5.842726	-0.027527	2.781387
140.532168	2535.380686	5.847731	-0.027583	2.785483
140.926713	2543.412099	5.852736	-0.027662	2.789579
141.007972	2551.467641	5.857741	-0.027682	2.793663
141.441027	2559.517973	5.862746	-0.027768	2.797759
141.721731	2567.555797	5.867750	-0.027826	2.801833
141.973312	2575.587142	5.872755	-0.027878	2.805897
142.276472	2583.631192	5.877760	-0.027939	2.809964
142.515021	2591.684523	5.882765	-0.027989	2.814026
142.741819	2599.745373	5.887770	-0.028036	2.818085
143.065984	2607.753895	5.892774	-0.028102	2.822118
143.498487	2615.774837	5.897779	-0.028188	2.826157
143.886401	2623.829446	5.902784	-0.028265	2.830205
143.986398	2631.917205	5.907789	-0.028289	2.834247
144.501862	2639.944448	5.912794	-0.028390	2.838276
144.897112	2647.935458	5.917798	-0.028469	2.842275
145.067000	2655.998587	5.922803	-0.028506	2.846292
145.221535	2664.061715	5.927808	-0.028540	2.850302
145.473982	2672.103844	5.932813	-0.028592	2.854301
145.809257	2680.141788	5.937818	-0.028659	2.858297
145.835963	2688.184657	5.942822	-0.028670	2.862273
146.113389	2696.223347	5.947827	-0.028726	2.866255
146.534360	2704.275733	5.952832	-0.028810	2.870246
146.869929	2712.319246	5.957837	-0.028878	2.874223
147.032965	2720.360229	5.962842	-0.028913	2.878183
147.112258	2728.405132	5.967846	-0.028933	2.882135
147.478497	2736.421025	5.972851	-0.029007	2.886083
147.673328	2744.479841	5.977856	-0.029048	2.890038
147.816900	2752.542686	5.982861	-0.029080	2.893986
148.066214	2760.578079	5.987866	-0.029132	2.897921
148.294707	2768.611445	5.992870	-0.029179	2.901848
148.399716	2776.621897	5.997875	-0.029204	2.905752
148.767844	2784.667027	6.002880	-0.029278	2.909682
148.978464	2792.806785	6.007885	-0.029322	2.913645
149.080313	2800.847821	6.012890	-0.029346	2.917548
149.335317	2808.806825	6.017894	-0.029399	2.921414
149.603918	2816.814454	6.022899	-0.029454	2.925299
149.907025	2824.821365	6.027904	-0.029516	2.929181
150.125998	2832.894849	6.032909	-0.029562	2.933085
150.456117	2840.946415	6.037914	-0.029629	2.936979
150.596333	2848.965066	6.042918	-0.029660	2.940842
150.998421	2856.944611	6.047923	-0.029740	2.944695
151.392593	2865.004079	6.052928	-0.029818	2.948581
151.425674	2873.096921	6.057933	-0.029830	2.952459
151.599980	2881.166328	6.062938	-0.029867	2.956327
151.728046	2889.146073	6.067942	-0.029896	2.960146
152.065738	2897.174674	6.072947	-0.029965	2.963993
152.446197	2905.203429	6.077952	-0.030041	2.967838
152.584832	2913.243623	6.082957	-0.030072	2.971671
153.208749	2921.307090	6.087962	-0.030193	2.975535
153.676757	2929.303801	6.092966	-0.030285	2.979353
153.801958	2937.361191	6.097971	-0.030314	2.983179
154.070672	2945.403920	6.102976	-0.030369	2.986999
154.403928	2953.404688	6.107981	-0.030436	2.990799
154.668249	2961.523645	6.112986	-0.030491	2.994645
155.024331	2969.515015	6.117990	-0.030562	2.998431
155.293833	2977.527096	6.122995	-0.030618	3.002218
155.557227	2985.566685	6.128000	-0.030672	3.006012
155.410360	2993.619584	6.133005	-0.030650	3.009788
155.910252	3001.676271	6.138010	-0.030748	3.013593
155.941594	3009.715557	6.143014	-0.030759	3.017361
156.252551	3017.736508	6.148019	-0.030822	3.021130
156.626565	3025.731691	6.153024	-0.030897	3.024885
156.746480	3033.802150	6.158029	-0.030924	3.028659
157.204958	3041.849745	6.163034	-0.031015	3.032433
157.353204	3049.894682	6.168038	-0.031048	3.036186
157.573867	3057.897196	6.173043	-0.031094	3.039918
157.880102	3065.938529	6.178048	-0.031156	3.043668
157.880122	3073.970866	6.183053	-0.031161	3.047395
158.147850	3082.067201	6.188058	-0.031216	3.051159
158.257363	3090.115601	6.193062	-0.031242	3.054889
158.424841	3098.103782	6.198067	-0.031278	3.058589
158.879933	3106.138079	6.203072	-0.031368	3.062319
159.152849	3114.144020	6.208077	-0.031424	3.066024
159.428794	3122.186618	6.213082	-0.031481	3.069740
159.720536	3130.300675	6.218086	-0.031540	3.073486
159.952274	3138.327494	6.223091	-0.031589	3.077184
160.101915	3146.344462	6.228096	-0.031622	3.080870
160.295324	3154.323085	6.233101	-0.031663	3.084536
160.847146	3162.325802	6.238106	-0.031771	3.088224
160.967761	3170.379558	6.243110	-0.031799	3.091912
161.249475	3178.420722	6.248115	-0.031856	3.095597
161.587457	3186.444768	6.253120	-0.031924	3.099272
161.968065	3194.446157	6.258125	-0.032000	3.102934
162.408722	3202.484181	6.263130	-0.032088	3.106612
162.467556	3210.532062	6.268134	-0.032104	3.110272
162.866804	3218.581884	6.273139	-0.032183	3.113944
163.113694	3226.639949	6.278144	-0.032235	3.117609
163.267291	3234.656823	6.283149	-0.032268	3.121246
163.641511	3242.660715	6.288154	-0.032343	3.124883
163.905247	3250.707113	6.293158	-0.032397	3.128530
164.009221	3258.777329	6.298163	-0.032422	3.132177
164.323161	3266.825367	6.303168	-0.032486	3.135818
164.092110	3274.847360	6.308173	-0.032448	3.139420
164.616454	3282.856205	6.313178	-0.032551	3.143045
164.805925	3290.882117	6.318182	-0.032591	3.146658
164.957160	3298.911323	6.323187	-0.032624	3.150267
165.198685	3306.994044	6.328192	-0.032675	3.153900
165.405621	3314.984883	6.333197	-0.032718	3.157486
165.757821	3323.014910	6.338202	-0.032789	3.161091
165.990948	3330.993017	6.343206	-0.032838	3.164665
166.217565	3339.057216	6.348211	-0.032885	3.168272
166.204112	3347.151652	6.353216	-0.032888	3.171878
166.526274	3355.155796	6.358221	-0.032953	3.175454
166.869392	3363.179777	6.363226	-0.033022	3.179036
166.854491	3371.212652	6.368230	-0.033024	3.182603
167.118742	3379.250512	6.373235	-0.033079	3.186179
167.501419	3387.263034	6.378240	-0.033155	3.189745
167.592109	3395.315210	6.383245	-0.033177	3.193313
168.240046	3403.338594	6.388250	-0.033303	3.196887
168.625860	3411.323157	6.393254	-0.033380	3.200429
168.795622	3419.377474	6.398259	-0.033417	3.203989
168.908837	3427.423466	6.403264	-0.033443	3.207538
169.019528	3435.446021	6.408269	-0.033469	3.211074
169.373261	3443.505899	6.413274	-0.033540	3.214632
169.528622	3451.531525	6.418278	-0.033574	3.218162
169.785727	3459.545174	6.423283	-0.033627	3.221688
170.227809	3467.557666	6.428288	-0.033715	3.225217
170.324084	3475.623376	6.433293	-0.033738	3.228751
170.552239	3483.715777	6.438298	-0.033786	3.232298
170.888921	3491.737066	6.443302	-0.033854	3.235815
171.053218	3499.717268	6.448307	-0.033889	3.239303
171.278657	3507.758598	6.453312	-0.033936	3.242816
171.203194	3515.789026	6.458317	-0.033928	3.246308
171.500499	3523.806857	6.463322	-0.033988	3.249807
171.652679	3531.824451	6.468326	-0.034022	3.253295
171.828422	3539.865142	6.473331	-0.034060	3.256791
172.049156	3547.880921	6.478336	-0.034106	3.260274
172.205136	3555.894674	6.483341	-0.034140	3.263749
172.592224	3563.915611	6.488346	-0.034217	3.267234
172.814309	3571.960949	6.493350	-0.034264	3.270718
172.936812	3579.999359	6.498355	-0.034292	3.274192
173.119576	3588.059061	6.503360	-0.034331	3.277674
173.308083	3596.045675	6.508365	-0.034371	3.281120
173.889231	3604.015756	6.513370	-0.034485	3.284571
174.302293	3612.056063	6.518374	-0.034567	3.288042
174.483358	3620.129418	6.523379	-0.034606	3.291515
174.715612	3628.192267	6.528384	-0.034654	3.294981
174.959328	3636.183956	6.533389	-0.034705	3.298414
175.283901	3644.217804	6.538394	-0.034770	3.301864
175.660380	3652.219823	6.543398	-0.034846	3.305299
175.833769	3660.244621	6.548403	-0.034883	3.308732
176.131938	3668.326171	6.553408	-0.034944	3.312191
175.972954	3676.394180	6.558413	-0.034919	3.315623
176.484901	3684.374970	6.563418	-0.035020	3.319039
176.693859	3692.390739	6.568422	-0.035064	3.322456
176.791460	3700.414291	6.573427	-0.035087	3.325868
177.119080	3708.445981	6.578432	-0.035154	3.329288
177.179206	3716.499021	6.583437	-0.035170	3.332704
177.342523	3724.568378	6.588442	-0.035206	3.336127
177.567925	3732.549186	6.593446	-0.035253	3.339512
177.893841	3740.521401	6.598451	-0.035319	3.342893
177.990390	3748.602241	6.603456	-0.035342	3.346308
178.010571	3756.619446	6.608461	-0.035351	3.349690
178.364493	3764.688821	6.613466	-0.035422	3.353103
178.556397	3772.727015	6.618470	-0.035463	3.356493
178.736364	3780.709823	6.623475	-0.035501	3.359856
178.948212	3788.741882	6.628480	-0.035546	3.363238
179.047649	3796.761160	6.633485	-0.035570	3.366606
179.329287	3804.793950	6.638490	-0.035627	3.369984
179.477775	3812.837245	6.643494	-0.035660	3.373357
179.649136	3820.865089	6.648499	-0.035697	3.376722
180.154912	3828.864673	6.653504	-0.035797	3.380083
180.294090	3836.895756	6.658509	-0.035828	3.383441
180.801607	3844.922020	6.663514	-0.035927	3.386807
180.751644	3852.983599	6.668518	-0.035923	3.390164
180.905092	3861.072968	6.673523	-0.035957	3.393537
181.338091	3869.090887	6.678528	-0.036043	3.396886
181.760551	3877.039614	6.683533	-0.036127	3.400203
182.809257	3884.999426	6.688538	-0.036327	3.403542
183.154174	3893.036962	6.693542	-0.036397	3.406887
183.406538	3901.076615	6.698547	-0.036449	3.410225
183.747404	3909.156255	6.703552	-0.036517	3.413580
183.819458	3917.195774	6.708557	-0.036536	3.416906
184.105572	3925.192386	6.713562	-0.036594	3.420218
184.661724	3933.177894	6.718566	-0.036703	3.423532
184.960633	3941.216589	6.723571	-0.036764	3.426855
185.248332	3949.258077	6.728576	-0.036823	3.430176
185.335029	3957.301759	6.733581	-0.036844	3.433488
185.616948	3965.348125	6.738586	-0.036902	3.436804
185.825398	3973.340614	6.743590	-0.036946	3.440092
185.805010	3981.384381	6.748595	-0.036947	3.443391
186.213178	3989.400730	6.753600	-0.037028	3.446689
186.369963	3997.423703	6.758605	-0.037063	3.449979
186.603809	4005.503251	6.763610	-0.037112	3.453291
187.036305	4013.507591	6.768614	-0.037197	3.456576
187.005905	4021.507539	6.773619	-0.037197	3.459841
187.409938	4029.522749	6.778624	-0.037277	3.463122
187.503532	4037.583319	6.783629	-0.037300	3.466410
187.729797	4045.613510	6.788634	-0.037347	3.469685
188.039704	4053.694753	6.793638	-0.037410	3.472982
188.336719	4061.694117	6.798643	-0.037470	3.476241
188.775823	4069.663084	6.803648	-0.037557	3.479489
188.603853	4077.702796	6.808653	-0.037531	3.482744
188.926821	4085.719915	6.813658	-0.037596	3.486002
189.332165	4093.749872	6.818662	-0.037677	3.489265
189.325382	4101.780060	6.823667	-0.037680	3.492512
189.972185	4109.812859	6.828672	-0.037806	3.495777
190.343025	4117.801991	6.833677	-0.037880	3.499013
190.350975	4125.844402	6.838682	-0.037887	3.502256
190.728106	4133.862103	6.843686	-0.037962	3.505498
191.230151	4141.849919	6.848691	-0.038061	3.508728
191.461064	4149.955343	6.853696	-0.038109	3.511995
191.424328	4157.995482	6.858701	-0.038108	3.515223
191.749508	4165.975858	6.863706	-0.038173	3.518436
191.981713	4174.015120	6.868710	-0.038222	3.521667
192.097335	4182.009863	6.873715	-0.038248	3.524873
192.176753	4190.063834	6.878720	-0.038268	3.528099
192.275544	4198.091742	6.883725	-0.038292	3.531312
192.753930	4206.102499	6.888730	-0.038386	3.534527
192.954594	4214.156386	6.893734	-0.038429	3.537748
192.971159	4222.177381	6.898739	-0.038437	3.540947
193.496290	4230.178838	6.903744	-0.038540	3.544150
193.579716	4238.214233	6.908749	-0.038561	3.547351
193.749842	4246.265447	6.913754	-0.038598	3.550558
194.012898	4254.405220	6.918758	-0.038652	3.553800
194.137079	4262.383368	6.923763	-0.038680	3.556971
194.536531	4270.337494	6.928768	-0.038760	3.560137
194.867498	4278.314932	6.933773	-0.038826	3.563308
195.010610	4286.400903	6.938778	-0.038858	3.566513
195.222251	4294.387374	6.943782	-0.038903	3.569678
195.448994	4302.430523	6.948787	-0.038950	3.572863
195.783488	4310.481870	6.953792	-0.039018	3.576052
195.706621	4318.483137	6.958797	-0.039009	3.579206
195.834236	4326.509218	6.963802	-0.039038	3.582373
195.919966	4334.537538	6.968806	-0.039059	3.585537
195.908307	4342.534713	6.973811	-0.039062	3.588683
196.207283	4350.595407	6.978816	-0.039123	3.591860
196.442652	4358.595536	6.983821	-0.039172	3.595008
196.850970	4366.595298	6.988826	-0.039253	3.598159
197.029147	4374.621734	6.993830	-0.039291	3.601310
197.185283	4382.590661	6.998835	-0.039325	3.604436
197.533360	4390.623309	7.003840	-0.039395	3.607589
197.445113	4398.665008	7.008845	-0.039384	3.610731
197.690294	4406.731923	7.013850	-0.039435	3.613890
197.982863	4414.744293	7.018854	-0.039495	3.617025
198.275047	4422.713326	7.023859	-0.039554	3.620141
198.525396	4430.770820	7.028864	-0.039606	3.623287
198.802759	4438.812712	7.033869	-0.039663	3.626425
199.083845	4446.812463	7.038874	-0.039720	3.629544
199.033751	4454.933630	7.043878	-0.039716	3.632699
199.406346	4462.922650	7.048883	-0.039791	3.635811
199.509385	4470.964497	7.053888	-0.039815	3.638934
199.581268	4478.985618	7.058893	-0.039834	3.642045
199.665407	4486.978125	7.063898	-0.039855	3.645143
200.154854	4494.979857	7.068902	-0.039951	3.648252
200.339040	4503.003627	7.073907	-0.039990	3.651359
200.467383	4511.061533	7.078912	-0.040020	3.654475
200.756614	4519.050830	7.083917	-0.040079	3.657566
200.942087	4527.103380	7.088922	-0.040118	3.660676
200.931792	4535.145148	7.093926	-0.040122	3.663774
201.373412	4543.121428	7.098931	-0.040209	3.666856
201.643079	4551.176135	7.103936	-0.040264	3.669962
201.527787	4559.246222	7.108941	-0.040248	3.673060
201.883466	4567.248056	7.113946	-0.040319	3.676142
202.283537	4575.205005	7.118950	-0.040399	3.679205
202.353275	4583.221414	7.123955	-0.040417	3.682280
202.600354	4591.240295	7.128960	-0.040468	3.685357
202.638210	4599.267407	7.133965	-0.040481	3.688430
202.876128	4607.310275	7.138970	-0.040530	3.691512
203.087919	4615.369847	7.143974	-0.040575	3.694596
203.140369	4623.389288	7.148979	-0.040590	3.697659
203.514554	4631.369282	7.153984	-0.040665	3.700712
203.616963	4639.362854	7.158989	-0.040689	3.703761
203.635742	4647.451264	7.163994	-0.040698	3.706842
203.918847	4655.454011	7.168998	-0.040755	3.709893
204.315463	4663.552377	7.174003	-0.040835	3.712982
204.608593	4671.599282	7.179008	-0.040894	3.716045
204.825415	4679.527769	7.184013	-0.040940	3.719059
205.394691	4687.521269	7.189018	-0.041051	3.722104
205.459159	4695.542607	7.194022	-0.041068	3.725145
205.508149	4703.569856	7.199027	-0.041082	3.728185
205.904391	4711.606752	7.204032	-0.041161	3.731235
206.096185	4719.649923	7.209037	-0.041202	3.734280
206.499468	4727.643612	7.214042	-0.041283	3.737308
206.730394	4735.655467	7.219046	-0.041331	3.740337
206.866109	4743.661578	7.224051	-0.041361	3.743358
206.869541	4751.771069	7.229056	-0.041367	3.746414
207.261825	4759.699891	7.234061	-0.041445	3.749407
207.768302	4767.746164	7.239066	-0.041545	3.752445
208.193036	4775.797522	7.244070	-0.041629	3.755481
208.240431	4783.767882	7.249075	-0.041643	3.758475
208.857738	4791.792537	7.254080	-0.041763	3.761500
209.080895	4799.778565	7.259085	-0.041810	3.764499
209.247131	4807.837022	7.264090	-0.041846	3.767521
209.652219	4815.902735	7.269094	-0.041927	3.770549
209.913100	4823.937801	7.274099	-0.041980	3.773560
210.117128	4832.011210	7.279104	-0.042024	3.776581
210.072331	4839.955385	7.284109	-0.042020	3.779547
210.273877	4847.996692	7.289114	-0.042063	3.782551
210.607499	4856.009054	7.294118	-0.042130	3.785546
210.728001	4864.027860	7.299123	-0.042158	3.788535
211.043041	4872.102084	7.304128	-0.042222	3.791547
211.179532	4880.126112	7.309133	-0.042253	3.794535
211.438095	4888.138504	7.314138	-0.042306	3.797518
211.542062	4896.135998	7.319142	-0.042330	3.800489
211.796704	4904.089851	7.324147	-0.042383	3.803446
212.180777	4912.179035	7.329152	-0.042460	3.806453
211.975445	4920.169499	7.334157	-0.042427	3.809409
212.490155	4928.210130	7.339162	-0.042528	3.812396
212.794497	4936.200889	7.344166	-0.042589	3.815358
212.909038	4944.242581	7.349171	-0.042616	3.818332
213.221608	4952.251483	7.354176	-0.042679	3.821296
213.426605	4960.283817	7.359181	-0.042723	3.824264
213.610787	4968.305021	7.364186	-0.042762	3.827225
213.949966	4976.323845	7.369190	-0.042831	3.830187
214.218872	4984.352952	7.374195	-0.042886	3.833148
214.551941	4992.395861	7.379200	-0.042953	3.836113
214.675728	5000.355625	7.384205	-0.042981	3.839041
215.010457	5008.384713	7.389210	-0.043049	3.841997
215.169241	5016.401733	7.394214	-0.043083	3.844942
215.243706	5024.407454	7.399219	-0.043102	3.847879
215.587966	5032.475340	7.404224	-0.043172	3.850842
215.851909	5040.507905	7.409229	-0.043226	3.853789
215.995688	5048.567769	7.414234	-0.043258	3.856740
216.113215	5056.560968	7.419238	-0.043285	3.859665
216.177640	5064.587086	7.424243	-0.043302	3.862598
216.525912	5072.612669	7.429248	-0.043372	3.865534
216.737047	5080.616734	7.434253	-0.043417	3.868457
216.943339	5088.671772	7.439258	-0.043460	3.871397
217.450084	5096.918631	7.444262	-0.043560	3.874410
217.647253	5104.840895	7.449267	-0.043602	3.877297
217.837444	5112.780687	7.454272	-0.043643	3.880187
217.996665	5120.803756	7.459277	-0.043677	3.883105
217.998713	5128.792118	7.464282	-0.043683	3.886006
218.241786	5136.795427	7.469286	-0.043733	3.888914
218.497717	5144.807618	7.474291	-0.043786	3.891823
219.008176	5152.854153	7.479296	-0.043886	3.894748
218.994611	5160.879583	7.484301	-0.043889	3.897652
219.092178	5168.860401	7.489306	-0.043912	3.900541
219.673478	5176.899377	7.494310	-0.044026	3.903457
219.685619	5184.893165	7.499315	-0.044033	3.906344
219.905328	5192.887548	7.504320	-0.044079	3.909233
219.942231	5200.932688	7.509325	-0.044091	3.912135
219.990180	5208.995402	7.514330	-0.044106	3.915042
220.314308	5217.006929	7.519334	-0.044171	3.917932
220.337059	5224.948423	7.524339	-0.044180	3.920790
220.762793	5232.957343	7.529344	-0.044265	3.923677
220.874853	5240.981801	7.534349	-0.044291	3.926562
221.139791	5249.002935	7.539354	-0.044345	3.929447
221.556867	5257.067880	7.544358	-0.044428	3.932348
221.520886	5265.067914	7.549363	-0.044427	3.935215
221.537631	5273.146184	7.554368	-0.044435	3.938109
221.807258	5281.100350	7.559373	-0.044490	3.940961
221.965190	5289.102471	7.564378	-0.044525	3.943826
222.306854	5297.163678	7.569382	-0.044594	3.946713
222.358570	5305.123301	7.574387	-0.044609	3.949557
222.615546	5313.248647	7.579392	-0.044662	3.952461
222.780474	5321.265370	7.584397	-0.044698	3.955323
222.914842	5329.285919	7.589402	-0.044728	3.958184
223.272633	5337.245673	7.594406	-0.044800	3.961025
223.311736	5345.238553	7.599411	-0.044812	3.963870
223.456288	5353.306039	7.604416	-0.044844	3.966741
224.023748	5361.256916	7.609421	-0.044955	3.969576
224.360596	5369.301817	7.614426	-0.045023	3.972438
224.261171	5377.389540	7.619430	-0.045010	3.975306
224.406642	5385.389014	7.624435	-0.045042	3.978145
224.888441	5393.375347	7.629440	-0.045137	3.980983
224.878742	5401.404110	7.634445	-0.045140	3.983825
225.000057	5409.411478	7.639450	-0.045168	3.986660
225.150744	5417.455077	7.644454	-0.045201	3.989507
225.207227	5425.512267	7.649459	-0.045217	3.992354
225.433482	5433.537559	7.654464	-0.045264	3.995191
225.830635	5441.561035	7.659469	-0.045343	3.998028
226.233374	5449.515725	7.664474	-0.045423	4.000839
226.450645	5457.540236	7.669478	-0.045469	4.003669
226.554706	5465.544459	7.674483	-0.045494	4.006489
227.079584	5473.573216	7.679488	-0.045596	4.009321
227.059571	5481.652085	7.684493	-0.045598	4.012161
227.000333	5489.687705	7.689498	-0.045592	4.014983
227.513825	5497.705982	7.694502	-0.045693	4.017806
227.648640	5505.673414	7.699507	-0.045723	4.020603
227.945010	5513.718828	7.704512	-0.045784	4.023428
228.157475	5521.724572	7.709517	-0.045828	4.026235
228.376861	5529.743737	7.714522	-0.045874	4.029046
228.598758	5537.839027	7.719526	-0.045921	4.031881
228.599566	5545.904741	7.724531	-0.045926	4.034700
228.980239	5553.876165	7.729536	-0.046002	4.037490
229.042162	5561.861180	7.734541	-0.046019	4.040279
229.317423	5569.844690	7.739546	-0.046075	4.043068
229.527227	5577.832057	7.744550	-0.046120	4.045855
229.769699	5585.842513	7.749555	-0.046170	4.048649
229.852690	5593.901016	7.754560	-0.046191	4.051455
230.132621	5601.927512	7.759565	-0.046248	4.054251
230.223342	5609.955654	7.764570	-0.046270	4.057043
230.203969	5617.971329	7.769574	-0.046272	4.059827
230.187949	5625.979777	7.774579	-0.046274	4.062607
230.723322	5633.966314	7.779584	-0.046379	4.065385
230.952731	5641.988708	7.784589	-0.046426	4.068169
230.702514	5650.037449	7.789594	-0.046385	4.070954
231.179396	5658.051299	7.794598	-0.046479	4.073735
231.315154	5666.071534	7.799603	-0.046509	4.076511
231.746141	5674.054195	7.804608	-0.046595	4.079277
231.761455	5682.092001	7.809613	-0.046603	4.082054
231.978121	5690.065119	7.814618	-0.046648	4.084809
232.262689	5698.121684	7.819622	-0.046707	4.087593
232.155146	5706.110946	7.824627	-0.046692	4.090346
232.479241	5714.184362	7.829632	-0.046757	4.093131
232.632712	5722.233575	7.834637	-0.046791	4.095905
232.881627	5730.199408	7.839642	-0.046843	4.098649
233.262620	5738.236609	7.844646	-0.046919	4.101417
233.475322	5746.189307	7.849651	-0.046963	4.104152
233.691885	5754.251864	7.854656	-0.047009	4.106923
233.882235	5762.250843	7.859661	-0.047050	4.109670
234.244692	5770.314549	7.864666	-0.047122	4.112440
234.689654	5778.376294	7.869670	-0.047210	4.115208
234.701815	5786.364455	7.874675	-0.047218	4.117943
235.109138	5794.349207	7.879680	-0.047299	4.120680
235.288483	5802.371342	7.884685	-0.047337	4.123426
235.476691	5810.361122	7.889690	-0.047378	4.126159
235.519738	5818.417202	7.894694	-0.047391	4.128910
235.535276	5826.451281	7.899699	-0.047399	4.131652
235.859411	5834.505558	7.904704	-0.047464	4.134403
235.911738	5842.560134	7.909709	-0.047479	4.137149
235.988974	5850.503695	7.914714	-0.047499	4.139856
236.227249	5858.530451	7.919718	-0.047548	4.142590
236.326961	5866.504921	7.924723	-0.047572	4.145304
236.624971	5874.605631	7.929728	-0.047633	4.148061
237.144715	5882.596804	7.934733	-0.047735	4.150782
237.311065	5890.633834	7.939738	-0.047771	4.153512
237.551010	5898.670089	7.944742	-0.047821	4.156241
237.547374	5906.650730	7.949747	-0.047825	4.158946
237.681852	5914.677183	7.954752	-0.047856	4.161667
237.969790	5922.646727	7.959757	-0.047914	4.164369
238.103813	5930.705971	7.964762	-0.047944	4.167097
238.506759	5938.728592	7.969766	-0.048025	4.169814
238.553097	5946.727444	7.974771	-0.048038	4.172517
238.794090	5954.793715	7.979776	-0.048089	4.175244
238.946211	5962.771947	7.984781	-0.048122	4.177938
239.312337	5970.782893	7.989786	-0.048195	4.180643
239.476376	5978.799053	7.994790	-0.048231	4.183347
239.526379	5986.806418	7.999795	-0.048246	4.186044
239.908187	5994.850429	8.004800	-0.048322	4.188755
240.059402	6002.885576	8.009805	-0.048355	4.191460
240.301775	6010.946415	8.014810	-0.048406	4.194172
240.451572	6019.042360	8.019814	-0.048439	4.196893
240.542792	6026.890503	8.024819	-0.048461	4.199529
240.739822	6034.942438	8.029824	-0.048503	4.202232
240.766603	6042.915310	8.034829	-0.048513	4.204905
240.660805	6050.914916	8.039834	-0.048498	4.207585
241.177488	6058.957199	8.044838	-0.048600	4.210283
241.481753	6066.984949	8.049843	-0.048661	4.212972
241.733978	6075.038152	8.054848	-0.048714	4.215667
241.887199	6083.031262	8.059853	-0.048747	4.218340
241.988535	6091.020715	8.064858	-0.048771	4.221009
242.255980	6099.014284	8.069862	-0.048826	4.223680
242.236301	6107.012727	8.074867	-0.048828	4.226348
242.515340	6115.069663	8.079872	-0.048885	4.229036
242.679279	6123.106935	8.084877	-0.048921	4.231715
242.764713	6131.141231	8.089882	-0.048942	4.234391
242.903454	6139.199835	8.094886	-0.048973	4.237073
243.120358	6147.142191	8.099891	-0.049018	4.239716
243.267903	6155.192982	8.104896	-0.049051	4.242392
243.594016	6163.146312	8.109901	-0.049117	4.245036
243.667258	6171.220659	8.114906	-0.049136	4.247717
243.969338	6179.229101	8.119910	-0.049197	4.250375
244.265654	6187.259800	8.124915	-0.049258	4.253040
244.157807	6195.283597	8.129920	-0.049243	4.255697
244.292403	6203.343820	8.134925	-0.049273	4.258366
244.621609	6211.304089	8.139930	-0.049339	4.261002
244.619202	6219.367637	8.144934	-0.049344	4.263668
244.787246	6227.325111	8.149939	-0.049381	4.266299
245.004823	6235.412115	8.154944	-0.049426	4.268971
245.453587	6243.398199	8.159949	-0.049515	4.271610
245.576999	6251.427768	8.164954	-0.049543	4.274259
245.626338	6259.504942	8.169958	-0.049558	4.276921
245.818784	6267.436725	8.174963	-0.049599	4.279535
245.880406	6275.530301	8.179968	-0.049615	4.282200
246.318612	6283.441449	8.184973	-0.049702	4.284806
246.460547	6291.500481	8.189978	-0.049734	4.287456
246.572117	6299.522508	8.194982	-0.049760	4.290093
246.810697	6307.544651	8.199987	-0.049809	4.292729
246.886418	6315.599397	8.204992	-0.049828	4.295372
246.830285	6323.638368	8.209997	-0.049823	4.298008
247.049086	6331.585470	8.215002	-0.049869	4.300615
247.463923	6339.586453	8.220006	-0.049951	4.303238
247.614902	6347.591726	8.225011	-0.049985	4.305860
247.854420	6355.599981	8.230016	-0.050035	4.308481
248.078274	6363.652727	8.235021	-0.050081	4.311116
248.345922	6371.678001	8.240026	-0.050136	4.313740
248.613016	6379.712115	8.245030	-0.050191	4.316365
248.779262	6387.689278	8.250035	-0.050227	4.318970
249.067795	6395.735765	8.255040	-0.050286	4.321596
249.117835	6403.709884	8.260045	-0.050301	4.324195
249.472655	6411.732336	8.265050	-0.050372	4.326811
249.733746	6419.767484	8.270054	-0.050426	4.329428
249.829141	6427.822511	8.275059	-0.050449	4.332049
249.997202	6435.842574	8.280064	-0.050485	4.334658
250.192631	6443.827591	8.285069	-0.050527	4.337254
250.270748	6451.826538	8.290074	-0.050547	4.339852
250.495976	6459.890934	8.295078	-0.050594	4.342471
250.519752	6467.809202	8.300083	-0.050603	4.345039
250.789656	6475.878685	8.305088	-0.050659	4.347657
250.942104	6483.920684	8.310093	-0.050692	4.350263
251.118649	6491.971943	8.315098	-0.050730	4.352871
251.358831	6500.037538	8.320102	-0.050780	4.355482
251.547315	6508.000871	8.325107	-0.050821	4.358059
251.761489	6515.959834	8.330112	-0.050866	4.360632
251.986360	6523.976577	8.335117	-0.050913	4.363223
252.145872	6531.983871	8.340122	-0.050948	4.365808
252.313618	6540.041337	8.345126	-0.050984	4.368409
252.479766	6548.016531	8.350131	-0.051020	4.370981
252.752020	6556.050876	8.355136	-0.051076	4.373571
252.924859	6564.105378	8.360141	-0.051113	4.376166
252.970111	6572.032983	8.365146	-0.051127	4.378717
253.402493	6580.111210	8.370150	-0.051213	4.381318
253.600321	6588.084622	8.375155	-0.051255	4.383882
253.661260	6596.148620	8.380160	-0.051271	4.386473
253.641069	6604.158419	8.385165	-0.051273	4.389045
253.911311	6612.161482	8.390170	-0.051328	4.391614
253.946537	6620.213942	8.395174	-0.051340	4.394197
253.968126	6628.247986	8.400179	-0.051349	4.396772
254.335613	6636.221985	8.405184	-0.051423	4.399328
254.438181	6644.271119	8.410189	-0.051447	4.401905
254.771879	6652.205411	8.415194	-0.051514	4.404445
254.837627	6660.325152	8.420198	-0.051532	4.407042
255.064505	6668.254853	8.425203	-0.051579	4.409577
255.268362	6676.346976	8.430208	-0.051622	4.412162
255.409264	6684.342092	8.435213	-0.051654	4.414714
255.780206	6692.391557	8.440218	-0.051728	4.417284
255.981072	6700.372777	8.445222	-0.051770	4.419829
255.846960	6708.408312	8.450227	-0.051751	4.422389
255.932106	6716.374917	8.455232	-0.051772	4.424926
256.162772	6724.464917	8.460237	-0.051820	4.427502
256.333116	6732.424035	8.465242	-0.051857	4.430034
256.491987	6740.509746	8.470246	-0.051891	4.432605
256.522579	6748.516317	8.475251	-0.051902	4.435149
256.815846	6756.535073	8.480256	-0.051962	4.437696
257.034648	6764.504358	8.485261	-0.052008	4.440226
257.219282	6772.512170	8.490266	-0.052048	4.442766
257.730306	6780.539521	8.495270	-0.052148	4.445313
257.798201	6788.547247	8.500275	-0.052166	4.447850
258.115316	6796.571536	8.505280	-0.052230	4.450391
258.433299	6804.646925	8.510285	-0.052294	4.452947
258.317135	6812.614345	8.515290	-0.052278	4.455467
258.682558	6820.668976	8.520294	-0.052351	4.458014
258.745749	6828.606011	8.525299	-0.052368	4.460521
258.981880	6836.676322	8.530304	-0.052417	4.463069
259.130445	6844.660191	8.535309	-0.052450	4.465589
259.107994	6852.686991	8.540314	-0.052451	4.468120
259.342833	6860.729688	8.545318	-0.052500	4.470655
259.503364	6868.738107	8.550323	-0.052535	4.473178
259.689387	6876.745919	8.555328	-0.052575	4.475699
259.838451	6884.766609	8.560333	-0.052608	4.478223
260.033676	6892.742809	8.565338	-0.052649	4.480732
260.239246	6900.772165	8.570343	-0.052693	4.483256
260.483267	6908.773985	8.575347	-0.052743	4.485769
260.500189	6916.794254	8.580352	-0.052752	4.488287
260.726859	6924.858124	8.585357	-0.052799	4.490817
260.795766	6932.846237	8.590362	-0.052817	4.493322
261.181489	6940.932026	8.595367	-0.052894	4.495857
261.159023	6948.873103	8.600371	-0.052895	4.498344
261.216867	6956.885816	8.605376	-0.052911	4.500852
261.496070	6964.918392	8.610381	-0.052968	4.503366
261.525348	6972.911395	8.615386	-0.052979	4.505865
261.765010	6980.968370	8.620391	-0.053029	4.508383
261.920588	6988.969519	8.625395	-0.053063	4.510882
262.161539	6997.032650	8.630400	-0.053113	4.513399
262.248559	7005.055304	8.635405	-0.053134	4.515902
262.377689	7012.978028	8.640410	-0.053163	4.518373
262.675670	7021.012385	8.645415	-0.053224	4.520877
262.702014	7028.982678	8.650419	-0.053234	4.523359
262.877639	7037.004703	8.655424	-0.053272	4.525857
263.089051	7045.064174	8.660429	-0.053317	4.528364
263.321163	7053.010583	8.665434	-0.053365	4.530835
263.357385	7061.145292	8.670439	-0.053377	4.533363
263.529449	7069.106954	8.675443	-0.053414	4.535836
263.705818	7077.133380	8.680448	-0.053452	4.538328
264.153478	7085.127892	8.685453	-0.053541	4.540808
264.286822	7093.134298	8.690458	-0.053571	4.543291
264.296514	7101.199039	8.695463	-0.053578	4.545790
264.355055	7109.214608	8.700467	-0.053594	4.548273
264.696252	7117.207359	8.705472	-0.053662	4.550747
265.011978	7125.291498	8.710477	-0.053726	4.553249
264.897775	7133.267436	8.715482	-0.053710	4.555715
265.005327	7141.277322	8.720487	-0.053736	4.558190
265.224833	7149.277150	8.725491	-0.053782	4.560661
265.533948	7157.274100	8.730496	-0.053844	4.563130
265.704549	7165.286971	8.735501	-0.053881	4.565602
265.895841	7173.316369	8.740506	-0.053922	4.568078
266.233648	7181.364105	8.745511	-0.053990	4.570559
266.312729	7189.394506	8.750515	-0.054010	4.573032
266.415827	7197.389693	8.755520	-0.054034	4.575494
266.618035	7205.421577	8.760525	-0.054077	4.577965
266.646829	7213.388023	8.765530	-0.054088	4.580415
266.949453	7221.495652	8.770535	-0.054149	4.582907
267.092754	7229.418855	8.775539	-0.054181	4.585341
267.227835	7237.460258	8.780544	-0.054212	4.587810
267.330865	7245.489783	8.785549	-0.054236	4.590274
267.418082	7253.568476	8.790554	-0.054257	4.592751
267.768718	7261.581279	8.795559	-0.054328	4.595207
267.770292	7269.585190	8.800563	-0.054333	4.597659
268.007691	7277.518004	8.805568	-0.054383	4.600088
268.170351	7285.621401	8.810573	-0.054418	4.602568
268.406593	7293.473025	8.815578	-0.054467	4.604970
268.600914	7301.580106	8.820583	-0.054509	4.607448
268.544812	7309.588106	8.825587	-0.054503	4.609895
268.826344	7317.643765	8.830592	-0.054561	4.612354
269.061880	7325.689446	8.835597	-0.054610	4.614810
269.165011	7333.667614	8.840602	-0.054634	4.617243
269.460584	7341.641200	8.845607	-0.054695	4.619674
269.536885	7349.680123	8.850611	-0.054714	4.622124
269.560931	7357.648372	8.855616	-0.054724	4.624551
269.970049	7365.726455	8.860621	-0.054805	4.627009
270.097083	7373.649120	8.865626	-0.054834	4.629419
270.294541	7381.773367	8.870631	-0.054876	4.631889
270.328788	7389.746358	8.875635	-0.054887	4.634312
270.519494	7397.808372	8.880640	-0.054928	4.636761
270.725687	7405.794549	8.885645	-0.054972	4.639185
270.843781	7413.816567	8.890650	-0.054999	4.641619
271.240232	7421.816143	8.895655	-0.055078	4.644045
271.119663	7429.881804	8.900659	-0.055060	4.646489
271.076814	7437.875729	8.905664	-0.055058	4.648911
271.343274	7445.888621	8.910669	-0.055112	4.651337
271.574443	7453.849917	8.915674	-0.055161	4.653746
271.698611	7461.902669	8.920679	-0.055189	4.656181
271.721821	7469.900296	8.925683	-0.055198	4.658599
272.187845	7477.887909	8.930688	-0.055290	4.661012
272.400611	7485.927057	8.935693	-0.055335	4.663439
272.303870	7493.936646	8.940698	-0.055322	4.665857
272.420707	7502.010624	8.945703	-0.055349	4.668292
272.593184	7510.011533	8.950707	-0.055387	4.670704
272.679454	7518.068959	8.955712	-0.055408	4.673132
273.025293	7526.119860	8.960717	-0.055477	4.675557
273.200050	7534.075391	8.965722	-0.055515	4.677951
273.345365	7542.029681	8.970727	-0.055547	4.680344
273.585840	7550.041739	8.975731	-0.055597	4.682753
273.941429	7558.001719	8.980736	-0.055669	4.685145
274.177208	7566.105350	8.985741	-0.055718	4.687579
274.115123	7574.056040	8.990746	-0.055711	4.689966
274.435060	7582.157370	8.995751	-0.055776	4.692397
274.461484	7590.127403	9.000755	-0.055786	4.694787
274.640987	7598.164238	9.005760	-0.055825	4.697196
274.982546	7606.180592	9.010765	-0.055894	4.699597
275.198880	7614.195932	9.015770	-0.055939	4.701997
275.322176	7622.123869	9.020775	-0.055967	4.704370
275.131582	7630.188720	9.025779	-0.055937	4.706783
275.570608	7638.224823	9.030784	-0.056024	4.709185
275.784324	7646.247407	9.035789	-0.056069	4.711582
275.538971	7654.276015	9.040794	-0.056028	4.713981
275.922081	7662.322128	9.045799	-0.056105	4.716382
276.277282	7670.250824	9.050803	-0.056176	4.718747
276.378389	7678.305641	9.055808	-0.056200	4.721149
276.515918	7686.313655	9.060813	-0.056231	4.723536
276.789029	7694.305211	9.065818	-0.056287	4.725916
277.051982	7702.384691	9.070823	-0.056341	4.728321
276.998434	7710.351597	9.075827	-0.056336	4.730693
277.149535	7718.426604	9.080832	-0.056370	4.733094
277.487814	7726.474306	9.085837	-0.056438	4.735486
277.650065	7734.432756	9.090842	-0.056473	4.737851
277.773857	7742.428440	9.095847	-0.056501	4.740225
277.922571	7750.482131	9.100851	-0.056534	4.742616
277.931274	7758.455107	9.105856	-0.056541	4.744982
278.060860	7766.569395	9.110861	-0.056570	4.747388
278.098761	7774.486551	9.115866	-0.056583	4.749735
278.468995	7782.521505	9.120871	-0.056657	4.752114
278.559137	7790.572818	9.125875	-0.056679	4.754498
278.738362	7798.576638	9.130880	-0.056717	4.756866
279.308038	7806.590801	9.135885	-0.056829	4.759235
279.144320	7814.551707	9.140890	-0.056803	4.761590
279.415303	7822.522482	9.145895	-0.056859	4.763944
279.808901	7830.603684	9.150899	-0.056937	4.766330
279.894160	7838.575786	9.155904	-0.056958	4.768683
279.945757	7846.681544	9.160909	-0.056973	4.771075
280.187529	7854.644882	9.165914	-0.057023	4.773423
280.387195	7862.714370	9.170919	-0.057066	4.775801
280.632968	7870.664656	9.175923	-0.057117	4.778142
280.668552	7878.689984	9.180928	-0.057128	4.780505
280.987519	7886.693949	9.185933	-0.057193	4.782860
281.022612	7894.672104	9.190938	-0.057205	4.785207
281.232170	7902.759949	9.195943	-0.057249	4.787585
281.406048	7910.727027	9.200947	-0.057286	4.789926
281.468612	7918.790888	9.205952	-0.057303	4.792294
281.853378	7926.775758	9.210957	-0.057380	4.794637
281.725559	7934.816872	9.215962	-0.057361	4.796997
282.079328	7942.810340	9.220967	-0.057433	4.799341
282.416119	7950.856565	9.225971	-0.057500	4.801698
282.434720	7958.763973	9.230976	-0.057509	4.804015
282.657770	7966.829077	9.235981	-0.057556	4.806376
282.673983	7974.819953	9.240986	-0.057564	4.808716
282.883106	7982.889651	9.245991	-0.057608	4.811076
283.008831	7990.400293	9.250995	-0.057636	4.813272
283.319377	7995.016815	9.256000	-0.057697	4.814620

283.275630	7997.361514	9.261005	-0.057690	4.815306
283.161775	7998.673328	9.266010	-0.057670	4.815690
283.501772	7999.486016	9.271015	-0.057734	4.815925
283.430240	7999.724015	9.276019	-0.057721	4.815995
283.365668	7999.702543	9.281024	-0.057709	4.815989
283.704839	7999.770645	9.286029	-0.057772	4.816007
283.670101	7999.698434	9.291034	-0.057765	4.815986
283.881616	7999.734311	9.296039	-0.057805	4.815996
283.911453	7999.835269	9.301043	-0.057810	4.816025
283.817466	7999.939326	9.306048	-0.057793	4.816056
283.923610	7999.930562	9.311053	-0.057812	4.816053
284.191538	7999.934345	9.316058	-0.057862	4.816053
284.203179	7999.867246	9.321063	-0.057864	4.816033
284.157106	7999.964694	9.326067	-0.057856	4.816062
283.937333	7999.801525	9.331072	-0.057815	4.816015
284.147399	7999.876905	9.336077	-0.057854	4.816036
284.145752	7999.991183	9.341082	-0.057853	4.816069
284.156660	7999.879201	9.346087	-0.057855	4.816037
284.182859	8000.053811	9.351091	-0.057860	4.816088
284.254117	7999.974972	9.356096	-0.057873	4.816064
284.390383	7999.885560	9.361101	-0.057899	4.816037
284.506269	7999.960304	9.366106	-0.057920	4.816059
284.639747	7999.821697	9.371111	-0.057945	4.816017
284.409376	7999.916873	9.376115	-0.057902	4.816046
284.384035	7999.854445	9.381120	-0.057897	4.816028
284.583485	7999.871944	9.386125	-0.057934	4.816032
284.628811	7999.896265	9.391130	-0.057943	4.816039
284.667963	7999.783725	9.396135	-0.057950	4.816006
284.783501	7999.920427	9.401139	-0.057972	4.816045
284.931660	7999.883579	9.406144	-0.057999	4.816034
284.831461	7999.846503	9.411149	-0.057980	4.816024
284.639535	7999.878275	9.416154	-0.057945	4.816034
284.813712	7999.863266	9.421159	-0.057977	4.816029
285.009513	7999.875358	9.426163	-0.058013	4.816031
284.774823	7999.954430	9.431168	-0.057970	4.816055
284.828140	7999.911590	9.436173	-0.057980	4.816043
284.852977	7999.966522	9.441178	-0.057984	4.816059
284.901731	7999.849882	9.446183	-0.057993	4.816024
284.929263	7999.920888	9.451187	-0.057998	4.816045
284.918727	7999.895052	9.456192	-0.057996	4.816037
284.879892	7999.915711	9.461197	-0.057989	4.816044
284.880212	7999.871910	9.466202	-0.057989	4.816031
285.176724	7999.792880	9.471207	-0.058044	4.816006
285.376607	7999.888378	9.476211	-0.058081	4.816033
285.117383	7999.963801	9.481216	-0.058033	4.816056
285.212850	7999.869375	9.486221	-0.058051	4.816028
285.365961	7999.967231	9.491226	-0.058079	4.816056
285.221893	7999.769104	9.496231	-0.058052	4.815999
285.162426	7999.965669	9.501235	-0.058041	4.816057
285.300559	7999.889110	9.506240	-0.058067	4.816034
285.631033	7999.852362	9.511245	-0.058128	4.816021
285.329715	8000.000740	9.516250	-0.058072	4.816066
285.510055	7999.849091	9.521255	-0.058106	4.816021
285.621015	7999.916270	9.526259	-0.058126	4.816040
285.240224	8000.016197	9.531264	-0.058056	4.816071
285.409235	7999.792764	9.536269	-0.058087	4.816005
285.642161	7999.968990	9.541274	-0.058130	4.816055
285.725599	7999.793149	9.546279	-0.058146	4.816003
285.542854	7999.941539	9.551283	-0.058112	4.816048
285.608569	7999.769651	9.556288	-0.058124	4.815997
285.773458	7999.938234	9.561293	-0.058154	4.816045
285.407062	7999.809791	9.566298	-0.058086	4.816010
285.543269	7999.887042	9.571303	-0.058111	4.816032
285.539578	7999.874150	9.576307	-0.058111	4.816028
285.722639	7999.843277	9.581312	-0.058145	4.816018
285.682265	7999.801943	9.586317	-0.058137	4.816006
285.563691	7999.879916	9.591322	-0.058115	4.816030
285.758346	7999.889851	9.596327	-0.058151	4.816031
285.460208	7999.892988	9.601331	-0.058096	4.816034
285.524179	7999.822563	9.606336	-0.058108	4.816013
285.750312	7999.866188	9.611341	-0.058150	4.816025
285.618249	7999.868062	9.616346	-0.058125	4.816026
285.524281	7999.794774	9.621351	-0.058107	4.816005
285.593203	7999.948796	9.626355	-0.058120	4.816049
285.456347	7999.845883	9.631360	-0.058095	4.816020
285.691787	7999.872583	9.636365	-0.058139	4.816027
285.807025	7999.810566	9.641370	-0.058160	4.816008
285.886052	7999.862208	9.646375	-0.058175	4.816023
285.634948	7999.870471	9.651379	-0.058128	4.816026
285.687101	7999.815857	9.656384	-0.058137	4.816010
285.870050	7999.861904	9.661389	-0.058171	4.816023
285.763155	7999.903765	9.666394	-0.058152	4.816035
285.851332	7999.803864	9.671399	-0.058168	4.816006
286.104690	7999.868283	9.676403	-0.058215	4.816023
286.028621	7999.808138	9.681408	-0.058201	4.816006
285.937509	7999.929345	9.686413	-0.058184	4.816042
285.771435	7999.887867	9.691418	-0.058153	4.816031
286.067902	7999.791743	9.696423	-0.058208	4.816001
285.917323	7999.911871	9.701427	-0.058180	4.816037
285.900604	7999.818615	9.706432	-0.058177	4.816010
286.030684	7999.797465	9.711437	-0.058201	4.816003
285.953273	7999.941356	9.716442	-0.058187	4.816045
285.870752	7999.830881	9.721447	-0.058171	4.816014
285.869849	7999.852227	9.726451	-0.058171	4.816020
285.860320	7999.897990	9.731456	-0.058169	4.816033
285.839425	7999.852735	9.736461	-0.058165	4.816020
285.875089	7999.883292	9.741466	-0.058172	4.816029
285.885817	7999.785192	9.746471	-0.058174	4.816000
286.060754	7999.897334	9.751475	-0.058206	4.816032
286.060827	7999.856732	9.756480	-0.058206	4.816020
286.023799	7999.840031	9.761485	-0.058199	4.816015
286.079739	7999.773733	9.766490	-0.058210	4.815996
286.212630	7999.877634	9.771495	-0.058234	4.816025
286.326510	7999.822002	9.776499	-0.058255	4.816009
286.230416	7999.824529	9.781504	-0.058237	4.816010
286.239179	7999.831094	9.786509	-0.058239	4.816012
286.219198	7999.899103	9.791514	-0.058235	4.816032
286.295728	7999.818221	9.796519	-0.058249	4.816008
286.213545	7999.933180	9.801523	-0.058234	4.816042
286.107604	7999.859673	9.806528	-0.058214	4.816021
286.371014	7999.776838	9.811533	-0.058263	4.815995
286.571291	7999.872347	9.816538	-0.058301	4.816022
286.478403	7999.789460	9.821543	-0.058283	4.815998
286.391093	7999.864796	9.826547	-0.058267	4.816021
286.379891	7999.872067	9.831552	-0.058265	4.816023
286.399934	7999.807255	9.836557	-0.058269	4.816004
286.306366	7999.888888	9.841562	-0.058251	4.816028
286.336199	7999.908655	9.846567	-0.058257	4.816034
286.272065	7999.807059	9.851571	-0.058245	4.816005
286.389750	7999.786753	9.856576	-0.058266	4.815998
286.602642	7999.953006	9.861581	-0.058306	4.816045
286.466250	7999.784926	9.866586	-0.058281	4.815997
286.338204	7999.896917	9.871591	-0.058257	4.816030
286.327574	7999.852916	9.876595	-0.058255	4.816018
286.324553	7999.880635	9.881600	-0.058254	4.816026
286.394123	7999.812447	9.886605	-0.058267	4.816005
286.214319	7999.891447	9.891610	-0.058234	4.816030
286.398675	7999.760169	9.896615	-0.058268	4.815990
286.628456	7999.876513	9.901619	-0.058311	4.816023
286.392700	7999.886122	9.906624	-0.058267	4.816027
286.531328	7999.818118	9.911629	-0.058292	4.816006
286.359219	7999.891916	9.916634	-0.058260	4.816029
286.497072	7999.828172	9.921639	-0.058286	4.816010
286.499533	7999.898726	9.926643	-0.058286	4.816030
286.585109	7999.853264	9.931648	-0.058302	4.816016
286.685430	7999.876447	9.936653	-0.058321	4.816023
286.305102	7999.911212	9.941658	-0.058250	4.816035
286.561185	7999.870980	9.946663	-0.058298	4.816022
286.433629	7999.857978	9.951667	-0.058274	4.816019
286.353967	7999.828750	9.956672	-0.058259	4.816010
286.560883	7999.928654	9.961677	-0.058297	4.816039
286.585004	7999.791264	9.966682	-0.058302	4.815998
286.441431	7999.803613	9.971687	-0.058275	4.816003
286.527879	7999.928042	9.976691	-0.058291	4.816039
286.581577	7999.783710	9.981696	-0.058301	4.815996
286.684657	7999.924467	9.986701	-0.058320	4.816037
286.706200	7999.790235	9.991706	-0.058324	4.815997
286.740554	7999.835726	9.996711	-0.058331	4.816010
286.894152	7999.839576	10.001715	-0.058359	4.816011
286.762759	7999.867104	10.006720	-0.058335	4.816020
286.650105	7999.780653	10.011725	-0.058313	4.815995
286.704518	7999.895953	10.016730	-0.058324	4.816028
286.782793	7999.765956	10.021735	-0.058338	4.815990
286.508610	7999.930853	10.026739	-0.058287	4.816040
286.536729	7999.826656	10.031744	-0.058292	4.816009
286.659512	7999.854520	10.036749	-0.058315	4.816016
286.526537	7999.937575	10.041754	-0.058290	4.816041
286.729601	7999.790610	10.046759	-0.058328	4.815997
286.873244	7999.846631	10.051763	-0.058355	4.816013
286.526069	7999.817893	10.056768	-0.058290	4.816006
286.777325	7999.951723	10.061773	-0.058337	4.816044
286.960962	7999.838593	10.066778	-0.058371	4.816010
286.907332	7999.849369	10.071783	-0.058361	4.816014
286.913001	7999.939213	10.076787	-0.058362	4.816040
286.960734	7999.815071	10.081792	-0.058371	4.816003
286.881728	7999.868122	10.086797	-0.058356	4.816019
286.673890	7999.887852	10.091802	-0.058317	4.816026
286.728355	7999.793748	10.096807	-0.058327	4.815998
286.947478	7999.953705	10.101811	-0.058368	4.816044
286.816022	7999.760072	10.106816	-0.058343	4.815988
286.792328	7999.878230	10.111821	-0.058339	4.816023
286.679940	7999.932812	10.116826	-0.058318	4.816039
286.663248	7999.861991	10.121831	-0.058315	4.816019
286.734030	7999.829082	10.126835	-0.058328	4.816009
286.747438	7999.781242	10.131840	-0.058331	4.815995
286.910350	7999.900649	10.136845	-0.058361	4.816029
286.888703	7999.935509	10.141850	-0.058357	4.816039
286.757460	7999.808121	10.146855	-0.058332	4.816002
286.818550	7999.812430	10.151859	-0.058344	4.816003
286.780665	7999.883321	10.156864	-0.058337	4.816024
286.869425	7999.803728	10.161869	-0.058353	4.816000
286.751042	7999.887048	10.166874	-0.058331	4.816025
286.910021	7999.850397	10.171879	-0.058360	4.816014
286.956942	7999.913211	10.176883	-0.058369	4.816032
286.891097	7999.761367	10.181888	-0.058357	4.815988
287.000999	7999.846692	10.186893	-0.058377	4.816012
286.835409	7999.966550	10.191898	-0.058346	4.816048
287.081503	7999.853485	10.196903	-0.058392	4.816014
287.241840	7999.840363	10.201907	-0.058422	4.816009
287.025036	7999.914419	10.206912	-0.058382	4.816032
287.019556	7999.866237	10.211917	-0.058381	4.816018
287.121018	7999.772985	10.216922	-0.058399	4.815990
287.305251	7999.908806	10.221927	-0.058434	4.816029
286.978012	7999.850512	10.226931	-0.058373	4.816014
286.940250	7999.781445	10.231936	-0.058365	4.815994
287.049115	7999.878504	10.236941	-0.058386	4.816021
287.115250	7999.901067	10.241946	-0.058398	4.816028
286.821962	7999.798518	10.246951	-0.058343	4.815999
286.937971	7999.860448	10.251955	-0.058365	4.816017
286.830859	7999.911920	10.256960	-0.058345	4.816032
287.131105	7999.783812	10.261965	-0.058401	4.815993
287.031621	7999.886707	10.266970	-0.058382	4.816024
286.857094	7999.865373	10.271975	-0.058350	4.816019
286.861093	7999.923135	10.276979	-0.058350	4.816035
286.803347	7999.875073	10.281984	-0.058340	4.816022
287.200461	7999.795732	10.286989	-0.058413	4.815996
287.137405	7999.812747	10.291994	-0.058402	4.816002
287.003532	7999.897923	10.296999	-0.058377	4.816027
287.139162	7999.833069	10.302003	-0.058402	4.816008
287.113675	7999.819782	10.307008	-0.058397	4.816004
287.079225	7999.844794	10.312013	-0.058391	4.816011
286.926850	7999.916813	10.317018	-0.058362	4.816033
287.069811	7999.793331	10.322023	-0.058389	4.815996
287.111010	7999.851768	10.327027	-0.058396	4.816013
287.041865	7999.879356	10.332032	-0.058384	4.816022
286.988595	7999.839922	10.337037	-0.058374	4.816010
286.942461	7999.849765	10.342042	-0.058365	4.816014
287.026858	7999.811761	10.347047	-0.058381	4.816002
286.971182	7999.958186	10.352051	-0.058370	4.816045
286.848580	7999.787150	10.357056	-0.058347	4.815996
286.980124	7999.841883	10.362061	-0.058372	4.816011
286.954248	7999.879872	10.367066	-0.058367	4.816022
287.061362	7999.863648	10.372071	-0.058387	4.816017
287.170563	7999.849598	10.377075	-0.058407	4.816012
286.910785	7999.873728	10.382080	-0.058359	4.816021
287.097199	7999.842916	10.387085	-0.058393	4.816011
287.058244	7999.882804	10.392090	-0.058386	4.816023
287.044340	7999.801349	10.397095	-0.058383	4.815999
287.178567	7999.890321	10.402099	-0.058408	4.816024
287.168476	7999.894407	10.407104	-0.058406	4.816025
287.203141	7999.761480	10.412109	-0.058413	4.815986
287.210991	7999.909058	10.417114	-0.058414	4.816030
287.306769	7999.793267	10.422119	-0.058432	4.815995
287.369696	7999.856372	10.427123	-0.058444	4.816013
287.162801	7999.935949	10.432128	-0.058405	4.816038
287.236518	7999.850741	10.437133	-0.058419	4.816012
287.129907	7999.833845	10.442138	-0.058399	4.816008
287.124652	7999.856182	10.447143	-0.058398	4.816015
287.149246	7999.973080	10.452147	-0.058403	4.816049
287.039892	7999.871729	10.457152	-0.058382	4.816020
287.126381	7999.760043	10.462157	-0.058398	4.815986
287.250007	7999.988785	10.467162	-0.058421	4.816053
287.404528	7999.863374	10.472167	-0.058450	4.816015
287.358586	7999.900999	10.477171	-0.058441	4.816026
287.240898	7999.942664	10.482176	-0.058419	4.816039
287.315946	7999.768802	10.487181	-0.058433	4.815988
287.030372	7999.895030	10.492186	-0.058380	4.816026
287.165014	7999.887853	10.497191	-0.058405	4.816024
287.334827	7999.862083	10.502195	-0.058437	4.816015
287.366318	7999.804955	10.507200	-0.058442	4.815998
287.231693	7999.843108	10.512205	-0.058417	4.816010
287.091229	7999.902523	10.517210	-0.058391	4.816028
287.040818	7999.847115	10.522215	-0.058382	4.816012
287.202245	7999.919486	10.527219	-0.058412	4.816033
287.336333	7999.771268	10.532224	-0.058436	4.815989
287.228365	7999.925293	10.537229	-0.058416	4.816034
287.205231	7999.815891	10.542234	-0.058412	4.816002
287.339889	7999.796961	10.547239	-0.058437	4.815996
287.345599	7999.942364	10.552243	-0.058438	4.816039
287.391468	7999.826735	10.557248	-0.058447	4.816005
287.319250	7999.804052	10.562253	-0.058433	4.815998
287.269289	7999.956993	10.567258	-0.058424	4.816043
287.571316	7999.858832	10.572263	-0.058480	4.816013
287.519854	7999.811952	10.577267	-0.058470	4.816000
287.320740	8000.003855	10.582272	-0.058433	4.816057
287.409706	7999.790713	10.587277	-0.058450	4.815994
287.540800	7999.831550	10.592282	-0.058474	4.816005
287.484121	7999.860433	10.597287	-0.058463	4.816014
287.385474	7999.843681	10.602291	-0.058445	4.816010
287.348031	7999.878255	10.607296	-0.058438	4.816020
287.301489	7999.802617	10.612301	-0.058429	4.815998
287.098285	7999.845936	10.617306	-0.058391	4.816012
287.208979	7999.831914	10.622311	-0.058412	4.816007
287.308571	7999.846537	10.627315	-0.058431	4.816011
287.330231	7999.940946	10.632320	-0.058435	4.816038
287.301192	7999.804726	10.637325	-0.058429	4.815999
287.329851	7999.898193	10.642330	-0.058434	4.816026
287.276187	7999.828837	10.647335	-0.058424	4.816006
287.249110	7999.933046	10.652339	-0.058419	4.816036
287.315203	7999.810304	10.657344	-0.058431	4.816000
287.507078	7999.828739	10.662349	-0.058467	4.816005
287.360278	7999.886971	10.667354	-0.058440	4.816022
287.294183	7999.866535	10.672359	-0.058427	4.816017
287.352122	7999.865445	10.677363	-0.058438	4.816016
287.123057	7999.886927	10.682368	-0.058395	4.816024
287.350634	7999.817331	10.687373	-0.058438	4.816002
287.339993	7999.896196	10.692378	-0.058436	4.816025
287.295382	7999.747942	10.697383	-0.058427	4.815982
287.275521	7999.841597	10.702387	-0.058424	4.816010
287.233280	7999.884631	10.707392	-0.058416	4.816022
287.415607	7999.868703	10.712397	-0.058450	4.816017
287.231810	7999.838653	10.717402	-0.058415	4.816009
287.216855	7999.877909	10.722407	-0.058413	4.816020
287.399254	7999.871598	10.727411	-0.058446	4.816018
287.346983	7999.875987	10.732416	-0.058437	4.816019
287.236765	7999.841931	10.737421	-0.058416	4.816010
287.385703	7999.941854	10.742426	-0.058444	4.816038
287.330012	7999.808356	10.747431	-0.058433	4.816000
287.343086	7999.795768	10.752435	-0.058436	4.815996
287.255656	7999.890334	10.757440	-0.058419	4.816024
287.339989	7999.840576	10.762445	-0.058435	4.816009
287.281132	7999.825614	10.767450	-0.058424	4.816005
287.308072	7999.788704	10.772455	-0.058429	4.815994
287.401234	7999.828853	10.777459	-0.058446	4.816005
287.288535	7999.897319	10.782464	-0.058425	4.816026
287.383007	7999.862702	10.787469	-0.058443	4.816015
287.358661	7999.852640	10.792474	-0.058438	4.816012
287.325570	7999.916140	10.797479	-0.058432	4.816031
287.278258	7999.813778	10.802483	-0.058423	4.816001
287.304031	7999.915741	10.807488	-0.058428	4.816031
287.742068	7999.851032	10.812493	-0.058510	4.816010
287.484752	7999.867727	10.817498	-0.058462	4.816016
287.424723	7999.873044	10.822503	-0.058450	4.816018
287.617720	7999.892567	10.827507	-0.058486	4.816023
287.370595	7999.901968	10.832512	-0.058440	4.816027
287.249247	7999.829247	10.837517	-0.058418	4.816006
287.193893	7999.883796	10.842522	-0.058407	4.816022
287.461108	7999.791414	10.847527	-0.058457	4.815994
287.379015	7999.895693	10.852531	-0.058442	4.816025
287.281831	7999.842641	10.857536	-0.058423	4.816010
287.508001	7999.845672	10.862541	-0.058465	4.816010
287.534871	7999.948723	10.867546	-0.058471	4.816040
287.373243	7999.849628	10.872551	-0.058440	4.816011
287.434741	7999.909503	10.877555	-0.058452	4.816029
287.465667	7999.901512	10.882560	-0.058457	4.816026
287.540162	7999.840891	10.887565	-0.058471	4.816008
287.436867	7999.909528	10.892570	-0.058452	4.816029
287.302107	7999.769253	10.897575	-0.058427	4.815988
287.520788	7999.845868	10.902579	-0.058467	4.816010
287.344128	7999.895011	10.907584	-0.058435	4.816025
287.484597	7999.802466	10.912589	-0.058461	4.815997
287.673261	7999.937300	10.917594	-0.058496	4.816035
287.580778	7999.798860	10.922599	-0.058478	4.815995
287.568135	7999.873415	10.927603	-0.058476	4.816017
287.596640	7999.920939	10.932608	-0.058481	4.816031
287.405968	7999.871532	10.937613	-0.058446	4.816018
287.489302	7999.807867	10.942618	-0.058461	4.815999
287.671496	7999.890231	10.947623	-0.058495	4.816022
287.751297	7999.885264	10.952627	-0.058510	4.816020
287.674985	7999.812291	10.957632	-0.058496	4.815999
287.609608	7999.818579	10.962637	-0.058483	4.816001
287.658157	7999.947666	10.967642	-0.058493	4.816039
287.656277	7999.821554	10.972647	-0.058492	4.816002
287.691616	7999.900185	10.977651	-0.058499	4.816025
287.655123	7999.895245	10.982656	-0.058492	4.816023
287.602799	7999.839801	10.987661	-0.058482	4.816007
287.582968	7999.902474	10.992666	-0.058478	4.816026
287.465949	7999.812736	10.997671	-0.058456	4.816000
287.533083	7999.819292	11.002675	-0.058469	4.816002
287.452250	7999.885131	11.007680	-0.058454	4.816021
287.548402	7999.841997	11.012685	-0.058472	4.816008
287.521014	7999.832949	11.017690	-0.058466	4.816006
287.539067	7999.887761	11.022695	-0.058470	4.816022
287.804636	7999.891507	11.027699	-0.058519	4.816021
287.671530	7999.795066	11.032704	-0.058494	4.815994
287.593066	7999.880180	11.037709	-0.058480	4.816019
287.540178	7999.896311	11.042714	-0.058470	4.816024
287.472672	7999.844866	11.047719	-0.058457	4.816010
287.758626	7999.877829	11.052723	-0.058510	4.816018
287.661383	7999.886744	11.057728	-0.058492	4.816021
287.626166	7999.794217	11.062733	-0.058486	4.815994
287.534304	7999.844898	11.067738	-0.058469	4.816009
287.505173	7999.877486	11.072743	-0.058463	4.816019
287.783766	7999.850484	11.077747	-0.058515	4.816010
287.621233	7999.890267	11.082752	-0.058485	4.816022
287.699242	7999.798725	11.087757	-0.058499	4.815995
287.461723	7999.907663	11.092762	-0.058455	4.816028
287.523688	7999.833994	11.097767	-0.058466	4.816006
287.458252	7999.842418	11.102771	-0.058454	4.816009
287.389271	7999.852915	11.107776	-0.058441	4.816012
287.397743	7999.845585	11.112781	-0.058443	4.816010
287.667934	7999.898562	11.117786	-0.058493	4.816024
287.573760	7999.884028	11.122791	-0.058475	4.816020
287.575368	7999.891531	11.127795	-0.058476	4.816023
287.634156	7999.894730	11.132800	-0.058487	4.816023
287.592210	7999.815970	11.137805	-0.058479	4.816000
287.566944	7999.836876	11.142810	-0.058474	4.816007
287.503739	7999.934019	11.147815	-0.058462	4.816035
287.612872	7999.789621	11.152819	-0.058482	4.815993
287.496300	7999.894343	11.157824	-0.058461	4.816024
287.695151	7999.895810	11.162829	-0.058498	4.816023
287.756042	7999.859516	11.167834	-0.058509	4.816012
287.615870	7999.910389	11.172839	-0.058483	4.816028
287.628806	7999.884977	11.177843	-0.058485	4.816020
287.754227	7999.885112	11.182848	-0.058508	4.816020
287.637078	7999.817808	11.187853	-0.058487	4.816001
287.584916	7999.978189	11.192858	-0.058477	4.816048
287.657498	7999.842743	11.197863	-0.058490	4.816008
287.673321	7999.943458	11.202867	-0.058493	4.816037
287.732542	7999.837686	11.207872	-0.058504	4.816006
287.588718	7999.772035	11.212877	-0.058477	4.815988
287.742667	7999.922266	11.217882	-0.058506	4.816031
287.696294	7999.873341	11.222887	-0.058497	4.816017
287.892675	7999.861942	11.227891	-0.058534	4.816012
287.809619	7999.926673	11.232896	-0.058518	4.816032
287.992149	7999.823138	11.237901	-0.058552	4.816000
287.875943	7999.868035	11.242906	-0.058531	4.816014
287.733279	7999.852621	11.247911	-0.058504	4.816010
287.808260	7999.847567	11.252915	-0.058518	4.816009
287.632655	7999.946944	11.257920	-0.058485	4.816039
287.702689	7999.738801	11.262925	-0.058498	4.815977
287.838226	7999.917545	11.267930	-0.058523	4.816029
287.688350	7999.896657	11.272935	-0.058495	4.816024
287.970554	7999.848353	11.277939	-0.058548	4.816008
287.907094	7999.898481	11.282944	-0.058536	4.816023
287.908178	7999.771354	11.287949	-0.058536	4.815986
287.844725	7999.901614	11.292954	-0.058524	4.816024
287.721652	7999.820313	11.297959	-0.058501	4.816001
287.972477	7999.919950	11.302963	-0.058548	4.816029
287.775914	7999.876847	11.307968	-0.058511	4.816017
287.726334	7999.868463	11.312973	-0.058502	4.816015
287.746789	7999.910499	11.317978	-0.058506	4.816027
287.681727	7999.864440	11.322983	-0.058494	4.816014
287.542621	7999.820243	11.327987	-0.058468	4.816002
287.712300	7999.900244	11.332992	-0.058499	4.816025
287.802819	7999.819613	11.337997	-0.058516	4.816000
287.663340	7999.859815	11.343002	-0.058490	4.816013
287.451426	7999.898702	11.348007	-0.058451	4.816025
287.777900	7999.904621	11.353011	-0.058511	4.816025
287.589039	7999.921490	11.358016	-0.058476	4.816031
287.728191	7999.883410	11.363021	-0.058502	4.816020
287.816252	7999.883935	11.368026	-0.058518	4.816019
287.863693	7999.820687	11.373031	-0.058527	4.816000
287.819816	7999.859417	11.378035	-0.058519	4.816012
287.745739	7999.933927	11.383040	-0.058505	4.816034
287.792798	7999.830071	11.388045	-0.058514	4.816004
287.840632	7999.811703	11.393050	-0.058523	4.815998
287.655312	7999.872441	11.398055	-0.058488	4.816017
287.948220	7999.857452	11.403059	-0.058543	4.816011
287.819971	7999.885036	11.408064	-0.058519	4.816020
287.672157	7999.881281	11.413069	-0.058491	4.816019
287.731581	7999.815044	11.418074	-0.058502	4.816000
287.700125	7999.867890	11.423079	-0.058496	4.816015
287.842971	7999.822398	11.428083	-0.058523	4.816001
287.654066	7999.949313	11.433088	-0.058488	4.816039
287.822951	7999.859421	11.438093	-0.058519	4.816012
287.821700	7999.867941	11.443098	-0.058519	4.816015
287.583051	7999.843306	11.448103	-0.058474	4.816009
287.955488	7999.883181	11.453107	-0.058543	4.816018
288.041528	7999.854822	11.458112	-0.058559	4.816010
287.982360	7999.883660	11.463117	-0.058548	4.816018
288.012478	7999.941897	11.468122	-0.058554	4.816035
287.765591	7999.770738	11.473127	-0.058508	4.815986
287.919032	7999.909208	11.478131	-0.058536	4.816026
287.742795	7999.927374	11.483136	-0.058504	4.816032
287.935631	7999.880653	11.488141	-0.058539	4.816018
287.773645	7999.801851	11.493146	-0.058509	4.815995
287.792677	7999.860955	11.498151	-0.058513	4.816013
287.967865	7999.871608	11.503155	-0.058545	4.816015
288.012522	7999.937589	11.508160	-0.058554	4.816034
287.755801	7999.874162	11.513165	-0.058506	4.816017
287.581079	7999.863508	11.518170	-0.058473	4.816015
287.362036	7999.895855	11.523175	-0.058432	4.816025
287.769128	7999.892553	11.528179	-0.058508	4.816022
287.877357	7999.931908	11.533184	-0.058528	4.816033
287.865002	7999.849410	11.538189	-0.058526	4.816009
287.726701	7999.874675	11.543194	-0.058500	4.816017
287.659412	7999.895887	11.548199	-0.058487	4.816024
287.838974	7999.771998	11.553203	-0.058521	4.815986
288.037881	7999.914499	11.558208	-0.058558	4.816027
288.047849	7999.838817	11.563213	-0.058560	4.816005
287.978626	7999.986068	11.568218	-0.058547	4.816048
287.737517	7999.825697	11.573223	-0.058502	4.816003
287.651255	7999.863659	11.578227	-0.058486	4.816014
287.758963	7999.969246	11.583232	-0.058506	4.816045
287.669242	7999.842608	11.588237	-0.058489	4.816008
287.579881	7999.920045	11.593242	-0.058472	4.816031
287.653698	7999.813470	11.598247	-0.058486	4.816000
287.734199	7999.877963	11.603251	-0.058501	4.816018
287.918286	7999.898394	11.608256	-0.058535	4.816023
287.816279	7999.801449	11.613261	-0.058516	4.815995
288.025297	7999.906738	11.618266	-0.058555	4.816025
287.791933	7999.884335	11.623271	-0.058511	4.816020
288.022309	7999.920564	11.628275	-0.058554	4.816029
289.012542	7999.904345	11.633280	-0.058739	4.816019
287.960479	7999.926912	11.638285	-0.058543	4.816031
288.620461	7999.864096	11.643290	-0.058665	4.816009
287.939317	7999.878440	11.648295	-0.058539	4.816017
287.874042	7999.945630	11.653299	-0.058526	4.816037
288.374771	7999.843597	11.658304	-0.058620	4.816005
288.062857	7999.852889	11.663309	-0.058561	4.816009
287.878024	7999.871968	11.668314	-0.058527	4.816015
288.064266	7999.905259	11.673319	-0.058562	4.816024
288.204938	7999.904602	11.678323	-0.058588	4.816023
288.432398	7999.860647	11.683328	-0.058630	4.816009
288.412020	7999.810056	11.688333	-0.058626	4.815995
288.411727	7999.889111	11.693338	-0.058626	4.816018
288.253981	7999.946075	11.698343	-0.058597	4.816035
288.302657	7999.919175	11.703347	-0.058606	4.816027
288.195526	7999.833888	11.708352	-0.058586	4.816003
288.287566	7999.940261	11.713357	-0.058603	4.816033
288.263928	7999.862900	11.718362	-0.058598	4.816011
288.174656	7999.817470	11.723367	-0.058582	4.815998
288.424541	7999.878628	11.728371	-0.058628	4.816015
288.184979	7999.890301	11.733376	-0.058584	4.816019
288.063605	7999.899847	11.738381	-0.058561	4.816023
288.215844	7999.917564	11.743386	-0.058589	4.816027
288.190137	7999.885040	11.748391	-0.058584	4.816018
288.156424	7999.841686	11.753395	-0.058578	4.816005
287.973290	7999.906737	11.758400	-0.058544	4.816025
288.129540	7999.788836	11.763405	-0.058573	4.815990
288.037204	7999.907888	11.768410	-0.058556	4.816025
288.062958	7999.813261	11.773415	-0.058560	4.815997
288.085381	7999.929054	11.778419	-0.058565	4.816031
288.071050	7999.879642	11.783424	-0.058562	4.816017
288.034632	7999.800981	11.788429	-0.058555	4.815994
288.201819	7999.956797	11.793434	-0.058586	4.816039
287.919181	7999.857640	11.798439	-0.058533	4.816011
288.179841	7999.797192	11.803443	-0.058582	4.815992
287.995030	7999.914566	11.808448	-0.058548	4.816027
288.209912	7999.774224	11.813453	-0.058587	4.815985
288.160647	7999.967780	11.818458	-0.058578	4.816042
288.006007	7999.848510	11.823463	-0.058549	4.816008
288.174398	7999.877203	11.828467	-0.058581	4.816015
287.806068	7999.919662	11.833472	-0.058512	4.816030
287.880114	7999.800269	11.838477	-0.058526	4.815995
288.215172	7999.890751	11.843482	-0.058588	4.816019
287.953425	7999.885996	11.848487	-0.058539	4.816019
287.945520	7999.789690	11.853491	-0.058538	4.815991
287.825202	7999.954177	11.858496	-0.058516	4.816040
288.013824	7999.913790	11.863501	-0.058551	4.816027
287.739402	7999.922695	11.868506	-0.058499	4.816031
287.540875	7999.916951	11.873511	-0.058462	4.816030
287.991542	7999.911235	11.878515	-0.058546	4.816026
287.963290	7999.932087	11.883520	-0.058541	4.816033
287.959812	7999.813424	11.888525	-0.058540	4.815998
288.113204	7999.868556	11.893530	-0.058569	4.816013
288.036944	7999.892810	11.898535	-0.058555	4.816021
288.194606	7999.813397	11.903539	-0.058584	4.815997
288.190702	7999.936192	11.908544	-0.058583	4.816033
288.308758	7999.810118	11.913549	-0.058605	4.815995
288.292376	7999.919865	11.918554	-0.058602	4.816027
288.233305	7999.778824	11.923559	-0.058591	4.815986
288.238503	7999.913536	11.928563	-0.058592	4.816026
287.995340	7999.831123	11.933568	-0.058546	4.816003
288.309741	7999.910546	11.938573	-0.058605	4.816025
288.336202	7999.890722	11.943578	-0.058610	4.816019
288.149744	7999.797585	11.948583	-0.058575	4.815992
288.211747	7999.945081	11.953587	-0.058587	4.816035
288.317176	7999.841215	11.958592	-0.058606	4.816004
288.216692	7999.832976	11.963597	-0.058587	4.816002
288.158370	7999.941962	11.968602	-0.058577	4.816035
288.027793	7999.811376	11.973607	-0.058552	4.815997
288.346190	7999.879119	11.978611	-0.058611	4.816015
288.190035	7999.863459	11.983616	-0.058582	4.816011
288.027086	7999.842334	11.988621	-0.058552	4.816006
288.203206	7999.945959	11.993626	-0.058585	4.816035
287.884967	7999.831199	11.998631	-0.058525	4.816004
288.001164	7999.862151	12.003635	-0.058547	4.816012
287.884109	7999.985028	12.008640	-0.058525	4.816049
288.155647	7999.817934	12.013645	-0.058576	4.815998
288.119289	7999.954029	12.018650	-0.058569	4.816038
288.123404	7999.851530	12.023655	-0.058569	4.816008
288.273492	7999.900192	12.028659	-0.058597	4.816022
288.046650	7999.810596	12.033664	-0.058555	4.815997
287.964578	7999.871071	12.038669	-0.058540	4.816015
288.096852	7999.896973	12.043674	-0.058564	4.816022
288.137564	7999.899844	12.048679	-0.058572	4.816022
288.023312	7999.962940	12.053683	-0.058551	4.816041
287.893177	7999.908221	12.058688	-0.058526	4.816026
288.187903	7999.897539	12.063693	-0.058581	4.816021
288.168030	7999.889695	12.068698	-0.058577	4.816019
288.267558	7999.885086	12.073703	-0.058596	4.816017
288.335428	7999.823276	12.078707	-0.058608	4.815999
288.225495	7999.954831	12.083712	-0.058588	4.816038
288.208545	7999.823101	12.088717	-0.058585	4.816000
288.045810	7999.875702	12.093722	-0.058554	4.816016
288.155494	7999.821061	12.098727	-0.058575	4.815999
287.981821	7999.937569	12.103731	-0.058542	4.816034
288.105819	7999.790235	12.108736	-0.058565	4.815990
288.228572	7999.901438	12.113741	-0.058588	4.816022
288.039866	7999.867024	12.118746	-0.058553	4.816013
287.862775	7999.822137	12.123751	-0.058520	4.816001
288.129059	7999.906029	12.128755	-0.058570	4.816024
288.217349	7999.878779	12.133760	-0.058586	4.816016
288.027291	7999.878531	12.138765	-0.058551	4.816017
288.046788	7999.924822	12.143770	-0.058554	4.816030
288.284555	7999.803058	12.148775	-0.058598	4.815993
288.233223	7999.853407	12.153779	-0.058589	4.816008
288.045594	7999.945088	12.158784	-0.058554	4.816036
288.275851	7999.850966	12.163789	-0.058597	4.816007
288.220803	7999.900179	12.168794	-0.058586	4.816022
287.939210	7999.899338	12.173799	-0.058534	4.816023
288.007369	7999.882407	12.178803	-0.058546	4.816018
288.060315	7999.885500	12.183808	-0.058556	4.816019
288.027531	7999.861395	12.188813	-0.058550	4.816012
288.002287	7999.898328	12.193818	-0.058545	4.816023
287.943138	7999.884429	12.198823	-0.058534	4.816019
287.897765	7999.931680	12.203827	-0.058526	4.816033
288.052694	7999.861834	12.208832	-0.058555	4.816012
288.195443	7999.926390	12.213837	-0.058581	4.816030
288.378103	7999.807899	12.218842	-0.058615	4.815994
288.057594	7999.915331	12.223847	-0.058555	4.816027
288.336355	7999.847733	12.228851	-0.058607	4.816006
288.227080	7999.881003	12.233856	-0.058587	4.816016
288.006488	7999.847079	12.238861	-0.058546	4.816008
288.075834	8000.000051	12.243866	-0.058559	4.816052
288.044168	7999.880876	12.248871	-0.058553	4.816017
287.988851	7999.857430	12.253875	-0.058542	4.816011
288.006480	7999.928262	12.258880	-0.058546	4.816031
288.110757	7999.816896	12.263885	-0.058565	4.815998
288.254029	7999.866503	12.268890	-0.058592	4.816012
288.146947	7999.946825	12.273895	-0.058572	4.816036
288.230319	7999.902391	12.278899	-0.058587	4.816023
288.232316	7999.896012	12.283904	-0.058587	4.816021
288.343999	7999.861708	12.288909	-0.058608	4.816010
288.120990	7999.912146	12.293914	-0.058567	4.816026
288.046448	7999.872325	12.298919	-0.058553	4.816015
288.259841	7999.872988	12.303923	-0.058592	4.816014
288.310310	7999.917705	12.308928	-0.058602	4.816027
288.118901	7999.831958	12.313933	-0.058566	4.816003
288.342885	7999.890508	12.318938	-0.058608	4.816019
288.150874	7999.939372	12.323943	-0.058572	4.816034
287.912487	7999.810035	12.328947	-0.058527	4.815997
288.336015	7999.863659	12.333952	-0.058606	4.816011
288.084372	7999.868704	12.338957	-0.058559	4.816014
288.086198	7999.963823	12.343962	-0.058560	4.816041
288.095140	7999.791963	12.348967	-0.058561	4.815991
288.257911	7999.862224	12.353971	-0.058591	4.816011
288.105651	7999.975915	12.358976	-0.058563	4.816045
288.156007	7999.865708	12.363981	-0.058572	4.816012
288.504074	7999.862405	12.368986	-0.058637	4.816010
288.310259	7999.850335	12.373991	-0.058601	4.816007
288.377343	7999.848343	12.378995	-0.058613	4.816006
288.306402	7999.954963	12.384000	-0.058600	4.816038
288.344700	7999.794320	12.389005	-0.058607	4.815990
288.318839	7999.835515	12.394010	-0.058602	4.816003
288.168672	8000.002666	12.399015	-0.058575	4.816052
288.447837	7999.819684	12.404019	-0.058626	4.815997
288.300487	7999.833031	12.409024	-0.058599	4.816002
288.368628	7999.888754	12.414029	-0.058612	4.816018
288.482829	7999.890822	12.419034	-0.058633	4.816018
288.192801	7999.837474	12.424039	-0.058579	4.816004
288.326706	7999.973455	12.429043	-0.058604	4.816043
288.384989	7999.889033	12.434048	-0.058614	4.816018
288.475890	7999.804135	12.439053	-0.058631	4.815993
288.355530	7999.898105	12.444058	-0.058609	4.816021
288.334931	7999.865674	12.449063	-0.058605	4.816011
288.452561	7999.831478	12.454067	-0.058627	4.816001
288.503351	7999.933897	12.459072	-0.058636	4.816030
288.580278	7999.792118	12.464077	-0.058650	4.815989
288.737675	7999.968058	12.469082	-0.058680	4.816039
288.601642	7999.861945	12.474087	-0.058654	4.816009
288.339827	7999.876420	12.479091	-0.058606	4.816015
288.274290	7999.876295	12.484096	-0.058593	4.816015
288.320373	7999.939096	12.489101	-0.058602	4.816033
288.258697	7999.905919	12.494106	-0.058590	4.816024
288.455706	7999.842179	12.499111	-0.058627	4.816004
288.401407	7999.909569	12.504115	-0.058617	4.816024
288.225832	7999.888214	12.509120	-0.058584	4.816019
288.278924	7999.924432	12.514125	-0.058594	4.816029
288.563733	7999.850532	12.519130	-0.058647	4.816006
288.433841	7999.838554	12.524135	-0.058623	4.816003
288.414649	7999.853160	12.529139	-0.058619	4.816007
288.221868	7999.987485	12.534144	-0.058583	4.816048
288.824947	7999.827476	12.539149	-0.058695	4.815998
288.439230	7999.919836	12.544154	-0.058624	4.816027
288.188355	7999.885361	12.549159	-0.058577	4.816018
288.605966	7999.907895	12.554163	-0.058654	4.816022
288.638108	7999.911679	12.559168	-0.058660	4.816023
288.227654	7999.856145	12.564173	-0.058584	4.816009
288.393257	7999.932869	12.569178	-0.058615	4.816031
288.377534	7999.847104	12.574183	-0.058612	4.816006
288.462186	7999.930905	12.579187	-0.058628	4.816030
288.351055	7999.895762	12.584192	-0.058607	4.816020
288.298870	7999.898016	12.589197	-0.058597	4.816021
288.368241	7999.826617	12.594202	-0.058610	4.816000
288.153469	7999.941311	12.599207	-0.058570	4.816035
288.201954	7999.849232	12.604211	-0.058579	4.816007
288.360877	7999.910876	12.609216	-0.058608	4.816025
288.244151	7999.924780	12.614221	-0.058587	4.816029
288.328391	7999.886772	12.619226	-0.058602	4.816018
288.565541	7999.911373	12.624231	-0.058646	4.816024
288.709543	7999.834917	12.629235	-0.058673	4.816000
288.780561	7999.906719	12.634240	-0.058686	4.816021
288.637350	7999.860309	12.639245	-0.058660	4.816008
288.463280	7999.828297	12.644250	-0.058627	4.816000
288.337512	7999.887979	12.649255	-0.058604	4.816018
288.383925	7999.946513	12.654259	-0.058612	4.816035
288.476005	7999.861636	12.659264	-0.058629	4.816010
288.330942	7999.910284	12.664269	-0.058602	4.816025
288.587121	7999.849755	12.669274	-0.058650	4.816005
288.451216	7999.879336	12.674279	-0.058625	4.816015
288.522761	7999.867809	12.679283	-0.058638	4.816011
288.520055	7999.977805	12.684288	-0.058637	4.816043
288.556265	7999.829945	12.689293	-0.058644	4.816000
288.503934	7999.896302	12.694298	-0.058634	4.816020
288.542506	7999.911956	12.699303	-0.058641	4.816024
288.436304	7999.928187	12.704307	-0.058622	4.816029
288.550359	7999.904610	12.709312	-0.058643	4.816022
288.301512	7999.964195	12.714317	-0.058596	4.816040
288.433187	7999.974060	12.719322	-0.058621	4.816043
288.584228	7999.869953	12.724327	-0.058649	4.816011
288.552140	7999.916378	12.729331	-0.058643	4.816025
288.565503	7999.881357	12.734336	-0.058645	4.816015
288.440210	7999.827794	12.739341	-0.058622	4.816000
288.358682	7999.965206	12.744346	-0.058607	4.816040
288.365907	7999.872379	12.749351	-0.058608	4.816013
288.655304	7999.864806	12.754355	-0.058662	4.816010
288.484778	7999.898033	12.759360	-0.058630	4.816020
288.493145	7999.823390	12.764365	-0.058632	4.815998
288.791610	7999.897183	12.769370	-0.058687	4.816018
288.916927	7999.957150	12.774375	-0.058710	4.816035
288.788895	7999.922768	12.779379	-0.058686	4.816026
288.742578	7999.917649	12.784384	-0.058678	4.816025
288.725347	7999.836130	12.789389	-0.058675	4.816001
288.896631	7999.876630	12.794394	-0.058706	4.816012
288.600073	7999.930007	12.799399	-0.058651	4.816029
288.622181	7999.791506	12.804403	-0.058655	4.815988
288.857131	7999.965650	12.809408	-0.058699	4.816038
288.687169	7999.837551	12.814413	-0.058667	4.816001
288.595102	7999.924556	12.819418	-0.058650	4.816027
288.558654	7999.824525	12.824423	-0.058643	4.815998
288.502297	7999.926068	12.829427	-0.058633	4.816028
288.630097	7999.792692	12.834432	-0.058656	4.815989
288.752869	7999.898554	12.839437	-0.058679	4.816019
288.767149	7999.826155	12.844442	-0.058682	4.815998
288.574112	7999.928422	12.849447	-0.058646	4.816029
288.763756	7999.850659	12.854451	-0.058681	4.816005
288.881019	7999.861330	12.859456	-0.058703	4.816007
288.555412	7999.830841	12.864461	-0.058642	4.816000
288.733002	7999.970822	12.869466	-0.058675	4.816040
288.704514	7999.834607	12.874471	-0.058670	4.816000
288.562239	7999.880100	12.879475	-0.058643	4.816015
288.400672	7999.906011	12.884480	-0.058613	4.816023
288.416486	7999.866761	12.889485	-0.058616	4.816011
288.788803	7999.978223	12.894490	-0.058685	4.816042
288.504302	7999.805308	12.899495	-0.058632	4.815993
288.581540	7999.844101	12.904499	-0.058647	4.816004
288.546676	7999.965266	12.909504	-0.058640	4.816040
288.732809	7999.842564	12.914509	-0.058675	4.816003
288.704538	7999.868758	12.919514	-0.058669	4.816010
288.609713	7999.927933	12.924519	-0.058652	4.816028
288.660623	7999.861541	12.929523	-0.058661	4.816009
288.566471	7999.855554	12.934528	-0.058644	4.816007
288.568322	7999.875883	12.939533	-0.058644	4.816013
288.688040	7999.963528	12.944538	-0.058666	4.816038
288.461771	7999.815176	12.949543	-0.058624	4.815996
288.705638	7999.874089	12.954547	-0.058669	4.816012
288.919096	7999.931382	12.959552	-0.058709	4.816028
288.786745	7999.948207	12.964557	-0.058684	4.816033
288.589932	7999.857017	12.969562	-0.058648	4.816008
288.890515	7999.819731	12.974567	-0.058704	4.815995
288.855699	7999.837258	12.979571	-0.058697	4.816000
288.744838	7999.942086	12.984576	-0.058676	4.816032
288.559012	7999.907723	12.989581	-0.058642	4.816023
288.861227	7999.853371	12.994586	-0.058698	4.816005
288.884526	7999.891186	12.999591	-0.058702	4.816016
288.670883	7999.810375	13.004595	-0.058662	4.815994
288.708467	7999.876228	13.009600	-0.058669	4.816013
288.761792	7999.958393	13.014605	-0.058679	4.816036
288.832555	7999.893430	13.019610	-0.058692	4.816017
288.931065	7999.850339	13.024615	-0.058711	4.816004
288.782922	7999.873288	13.029619	-0.058683	4.816011
288.847319	7999.860562	13.034624	-0.058695	4.816007
288.654690	7999.816461	13.039629	-0.058659	4.815995
288.927146	7999.866276	13.044634	-0.058710	4.816009
288.785294	7999.910709	13.049639	-0.058683	4.816022
288.604678	7999.870030	13.054643	-0.058650	4.816011
288.760128	7999.793782	13.059648	-0.058678	4.815988
288.727950	7999.858369	13.064653	-0.058672	4.816007
288.672663	7999.916125	13.069658	-0.058662	4.816025
288.550604	7999.829498	13.074663	-0.058639	4.816000
288.574865	7999.906862	13.079667	-0.058644	4.816022
288.898740	7999.883889	13.084672	-0.058704	4.816014
288.718637	7999.876341	13.089677	-0.058671	4.816013
289.060623	7999.926351	13.094682	-0.058734	4.816025
288.737366	7999.808292	13.099687	-0.058674	4.815993
288.912123	7999.926852	13.104691	-0.058706	4.816026
288.899581	7999.867855	13.109696	-0.058704	4.816009
288.774726	7999.861310	13.114701	-0.058681	4.816008
288.904302	7999.864726	13.119706	-0.058705	4.816008
288.750073	7999.882223	13.124711	-0.058676	4.816014
288.965379	7999.853005	13.129715	-0.058716	4.816005
288.837755	7999.978897	13.134720	-0.058692	4.816042
288.573688	7999.828791	13.139725	-0.058643	4.816000
288.726563	7999.881778	13.144730	-0.058672	4.816014
288.544982	7999.944721	13.149735	-0.058638	4.816034
288.402471	7999.863065	13.154739	-0.058611	4.816010
288.752685	7999.844843	13.159744	-0.058676	4.816003
288.867467	7999.898208	13.164749	-0.058698	4.816018
288.622059	7999.865969	13.169754	-0.058652	4.816010
288.554969	7999.905347	13.174759	-0.058639	4.816022
288.591714	7999.866478	13.179763	-0.058646	4.816010
288.696462	7999.949576	13.184768	-0.058666	4.816034
288.612763	7999.809155	13.189773	-0.058650	4.815994
288.792130	7999.875444	13.194778	-0.058683	4.816012
288.944538	7999.927355	13.199783	-0.058712	4.816026
289.022663	7999.825130	13.204787	-0.058726	4.815996
288.974726	7999.923621	13.209792	-0.058717	4.816025
288.953625	7999.832415	13.214797	-0.058713	4.815999
288.943486	7999.865348	13.219802	-0.058711	4.816008
288.970370	7999.949171	13.224807	-0.058716	4.816033
288.920243	7999.812564	13.229811	-0.058707	4.815993
288.828461	7999.908122	13.234816	-0.058690	4.816021
288.646344	7999.891990	13.239821	-0.058656	4.816018
288.897947	7999.821761	13.244826	-0.058702	4.815996
288.886603	7999.959381	13.249831	-0.058700	4.816036
288.799090	7999.815684	13.254835	-0.058684	4.815995
288.745812	7999.942926	13.259840	-0.058674	4.816032
288.877797	7999.901511	13.264845	-0.058699	4.816019
289.000303	7999.866335	13.269850	-0.058721	4.816008
288.839241	7999.830285	13.274855	-0.058691	4.815999
288.938945	7999.872691	13.279859	-0.058710	4.816010
289.123320	7999.960442	13.284864	-0.058744	4.816035
288.832397	7999.870748	13.289869	-0.058690	4.816010
288.912756	7999.893572	13.294874	-0.058705	4.816017
288.875604	7999.867250	13.299879	-0.058698	4.816009
288.903701	7999.799375	13.304883	-0.058703	4.815989
289.099498	8000.007000	13.309888	-0.058740	4.816049
289.000290	7999.806462	13.314893	-0.058721	4.815991
288.864601	7999.848869	13.319898	-0.058696	4.816004
288.793825	7999.953356	13.324903	-0.058682	4.816035
288.939791	7999.802145	13.329907	-0.058709	4.815990
288.854213	7999.898884	13.334912	-0.058694	4.816019
288.737513	7999.882871	13.339917	-0.058672	4.816015
289.047176	7999.833997	13.344922	-0.058729	4.815999
289.002135	7999.928267	13.349927	-0.058721	4.816026
288.832125	7999.799100	13.354931	-0.058689	4.815990
288.976625	7999.887194	13.359936	-0.058716	4.816015
288.919676	7999.963084	13.364941	-0.058706	4.816037
289.012868	7999.875022	13.369946	-0.058723	4.816011
288.857330	7999.899973	13.374951	-0.058694	4.816019
289.060817	7999.871609	13.379955	-0.058732	4.816010
288.950224	7999.817243	13.384960	-0.058711	4.815994
288.833278	7999.901660	13.389965	-0.058689	4.816020
288.914636	7999.871079	13.394970	-0.058704	4.816010
288.998607	7999.932432	13.399975	-0.058720	4.816028
288.929091	7999.804020	13.404979	-0.058707	4.815990
289.082816	7999.883735	13.409984	-0.058735	4.816013
288.836985	7999.897431	13.414989	-0.058690	4.816018
288.898045	7999.887851	13.419994	-0.058701	4.816015
288.826770	7999.820309	13.424999	-0.058688	4.815996
288.795415	7999.874226	13.430003	-0.058682	4.816012
288.985797	7999.915073	13.435008	-0.058717	4.816023
288.970598	7999.889150	13.440013	-0.058714	4.816015
289.196341	7999.886833	13.445018	-0.058756	4.816013
289.137682	7999.860121	13.450023	-0.058745	4.816006
289.018321	7999.908167	13.455027	-0.058723	4.816020
288.971170	7999.872047	13.460032	-0.058714	4.816010
288.964006	7999.923198	13.465037	-0.058713	4.816025
289.026787	7999.826036	13.470042	-0.058724	4.815996
288.984789	7999.896855	13.475047	-0.058717	4.816017
288.987789	7999.836004	13.480051	-0.058717	4.816000
289.203802	7999.956383	13.485056	-0.058757	4.816034
289.021835	7999.860119	13.490061	-0.058723	4.816006
288.800701	7999.816568	13.495066	-0.058682	4.815995
288.899379	7999.889940	13.500071	-0.058700	4.816016
288.929725	7999.912924	13.505075	-0.058706	4.816022
288.895548	7999.830029	13.510080	-0.058700	4.815998
288.873022	7999.861669	13.515085	-0.058695	4.816008
289.180218	7999.903569	13.520090	-0.058753	4.816018
289.197843	7999.840845	13.525095	-0.058756	4.816000
289.208362	7999.899797	13.530099	-0.058758	4.816017
289.134502	7999.904862	13.535104	-0.058744	4.816019
288.972889	7999.876281	13.540109	-0.058714	4.816011
289.001170	7999.883200	13.545114	-0.058719	4.816013
288.826291	7999.857584	13.550119	-0.058686	4.816007
289.070850	7999.808597	13.555123	-0.058732	4.815991
289.065902	7999.915347	13.560128	-0.058731	4.816022
288.982895	7999.831565	13.565133	-0.058715	4.815998
289.107672	7999.888317	13.570138	-0.058739	4.816014
289.020238	7999.894204	13.575143	-0.058722	4.816016
289.010391	7999.911116	13.580147	-0.058720	4.816021
289.084680	7999.819505	13.585152	-0.058734	4.815994
289.114708	7999.865989	13.590157	-0.058740	4.816008
288.981178	7999.852876	13.595162	-0.058715	4.816005
289.064839	8000.025344	13.600167	-0.058730	4.816054
289.120554	7999.903478	13.605171	-0.058741	4.816019
289.032210	7999.832420	13.610176	-0.058724	4.815998
288.953267	7999.912185	13.615181	-0.058709	4.816022
288.954512	7999.806427	13.620186	-0.058710	4.815991
289.157536	7999.895584	13.625191	-0.058747	4.816016
288.944731	7999.889579	13.630195	-0.058708	4.816015
289.127579	7999.912126	13.635200	-0.058742	4.816021
289.082565	7999.894209	13.640205	-0.058733	4.816016
289.052973	7999.931064	13.645210	-0.058728	4.816027
288.964693	7999.894197	13.650215	-0.058711	4.816017
289.097457	7999.892330	13.655219	-0.058736	4.816015
289.103260	7999.824049	13.660224	-0.058737	4.815995
289.089641	7999.990477	13.665229	-0.058734	4.816044
289.337467	7999.801581	13.670234	-0.058780	4.815988
289.109200	7999.984412	13.675239	-0.058738	4.816042
289.001452	7999.880948	13.680243	-0.058718	4.816013
289.096668	7999.835660	13.685248	-0.058735	4.815999
289.010884	7999.931328	13.690253	-0.058720	4.816027
289.196969	7999.867389	13.695258	-0.058754	4.816008
289.109239	7999.912804	13.700263	-0.058738	4.816021
289.271448	7999.776845	13.705267	-0.058768	4.815981
289.260014	7999.932628	13.710272	-0.058766	4.816026
288.958530	7999.873727	13.715277	-0.058709	4.816011
289.131008	7999.790309	13.720282	-0.058742	4.815985
289.057533	7999.894748	13.725287	-0.058728	4.816016
289.026493	7999.881358	13.730291	-0.058722	4.816013
288.938692	7999.879760	13.735296	-0.058706	4.816013
289.098718	7999.873044	13.740301	-0.058735	4.816010
289.093149	7999.880418	13.745306	-0.058734	4.816012
289.033202	7999.817355	13.750311	-0.058723	4.815994
289.177208	7999.896894	13.755315	-0.058750	4.816016
289.177851	7999.903311	13.760320	-0.058750	4.816018
288.983302	7999.793998	13.765325	-0.058714	4.815987
289.108918	7999.947995	13.770330	-0.058737	4.816032
289.041898	7999.810011	13.775335	-0.058724	4.815992
289.102535	7999.906200	13.780339	-0.058736	4.816020
289.166558	7999.858209	13.785344	-0.058748	4.816005
289.229149	7999.912764	13.790349	-0.058759	4.816021
289.308377	7999.861843	13.795354	-0.058774	4.816005
289.026014	7999.871671	13.800359	-0.058721	4.816010
289.091044	7999.895285	13.805363	-0.058733	4.816016
289.335810	7999.869807	13.810368	-0.058779	4.816008
289.137638	7999.889711	13.815373	-0.058742	4.816015
289.189881	7999.831890	13.820378	-0.058752	4.815997
289.310980	7999.974052	13.825383	-0.058774	4.816038
289.197214	7999.868341	13.830387	-0.058753	4.816008
289.371698	7999.900353	13.835392	-0.058785	4.816016
289.413039	7999.948112	13.840397	-0.058793	4.816030
289.197439	7999.857648	13.845402	-0.058753	4.816005
289.089945	7999.846076	13.850407	-0.058733	4.816002
289.292531	7999.925610	13.855411	-0.058770	4.816024
289.387279	7999.871766	13.860416	-0.058788	4.816008
289.110612	7999.923366	13.865421	-0.058736	4.816025
289.173610	7999.883904	13.870426	-0.058748	4.816013
289.312919	7999.868265	13.875431	-0.058774	4.816007
289.179805	7999.916061	13.880435	-0.058749	4.816022
289.189684	7999.880977	13.885440	-0.058751	4.816012
289.088792	7999.847087	13.890445	-0.058732	4.816002
289.244975	7999.883040	13.895450	-0.058761	4.816012
289.179007	7999.901071	13.900455	-0.058749	4.816018
289.124413	7999.933197	13.905459	-0.058739	4.816027
289.114981	7999.868914	13.910464	-0.058737	4.816009
289.126001	7999.956723	13.915469	-0.058739	4.816034
289.260250	7999.904665	13.920474	-0.058764	4.816018
289.223585	7999.881557	13.925479	-0.058757	4.816012
289.220100	7999.802424	13.930483	-0.058756	4.815989
289.245304	7999.962077	13.935488	-0.058761	4.816035
289.332665	7999.825827	13.940493	-0.058777	4.815995
289.434644	7999.861865	13.945498	-0.058796	4.816005
289.287163	7999.964960	13.950503	-0.058769	4.816036
289.310207	7999.806174	13.955507	-0.058773	4.815989
289.248708	7999.902282	13.960512	-0.058761	4.816018
289.134751	7999.933331	13.965517	-0.058740	4.816027
289.258417	7999.828726	13.970522	-0.058763	4.815996
289.148293	7999.842749	13.975527	-0.058742	4.816001
289.009404	7999.878688	13.980531	-0.058717	4.816012
289.172699	7999.971398	13.985536	-0.058747	4.816038
289.072948	7999.865943	13.990541	-0.058728	4.816008
289.152817	7999.834266	13.995546	-0.058743	4.815998
288.972946	7999.962416	14.000551	-0.058710	4.816037
288.947650	7999.827327	14.005555	-0.058705	4.815997
289.057832	7999.944716	14.010560	-0.058725	4.816031
289.025067	7999.930227	14.015565	-0.058719	4.816027
288.983278	7999.918779	14.020570	-0.058711	4.816024
288.982132	7999.957218	14.025575	-0.058711	4.816035
289.078291	7999.874551	14.030579	-0.058729	4.816010
289.282332	7999.904963	14.035584	-0.058767	4.816018
289.139017	7999.873508	14.040589	-0.058740	4.816010
289.358020	7999.873206	14.045594	-0.058781	4.816009
289.330943	7999.962461	14.050599	-0.058776	4.816035
289.308798	7999.870166	14.055603	-0.058772	4.816008
289.194606	7999.938607	14.060608	-0.058750	4.816029
288.915865	7999.923926	14.065613	-0.058698	4.816026
288.782650	7999.978130	14.070618	-0.058674	4.816042
288.441916	7999.980488	14.075623	-0.058610	4.816045
288.860006	7999.941062	14.080627	-0.058688	4.816031
288.827772	7999.931924	14.085632	-0.058682	4.816029
288.728467	7999.998498	14.090637	-0.058663	4.816049
289.021955	7999.989932	14.095642	-0.058718	4.816045
289.101202	7999.933670	14.100647	-0.058733	4.816028
289.304622	7999.879662	14.105651	-0.058770	4.816011
289.329976	7999.891871	14.110656	-0.058775	4.816014
289.294096	7999.853819	14.115661	-0.058768	4.816003
289.271503	7999.964524	14.120666	-0.058764	4.816036
289.309498	7999.867980	14.125671	-0.058771	4.816007
289.273345	7999.810691	14.130675	-0.058764	4.815991
289.253693	7999.956708	14.135680	-0.058761	4.816034
289.239991	7999.810076	14.140685	-0.058758	4.815991
289.304588	7999.927706	14.145690	-0.058770	4.816025
289.434267	7999.863812	14.150695	-0.058794	4.816005
289.447432	7999.892895	14.155699	-0.058797	4.816014
289.542955	7999.827312	14.160704	-0.058814	4.815994
289.361580	7999.973599	14.165709	-0.058780	4.816038
289.381975	7999.950459	14.170714	-0.058784	4.816031
289.248543	7999.902087	14.175719	-0.058759	4.816018
289.405171	7999.855778	14.180723	-0.058788	4.816003
289.382787	7999.914132	14.185728	-0.058784	4.816020
289.247211	7999.976842	14.190733	-0.058759	4.816040
289.324378	7999.826518	14.195738	-0.058773	4.815995
289.450304	7999.906797	14.200743	-0.058797	4.816018
289.330880	7999.845859	14.205747	-0.058774	4.816001
289.391210	7999.872593	14.210752	-0.058786	4.816008
289.336005	7999.959200	14.215757	-0.058775	4.816034
289.317958	7999.833858	14.220762	-0.058772	4.815997
289.415281	7999.912549	14.225767	-0.058790	4.816020
289.468658	7999.860091	14.230771	-0.058800	4.816004
289.456898	7999.891927	14.235776	-0.058798	4.816014
289.234083	7999.909246	14.240781	-0.058756	4.816020
289.290151	7999.858974	14.245786	-0.058766	4.816005
289.321238	7999.939668	14.250791	-0.058772	4.816028
289.249364	7999.796254	14.255795	-0.058759	4.815987
289.392707	7999.698417	14.260800	-0.058785	4.815957

289.466192	7996.363315	14.265805	-0.058797	4.814982
289.425705	7990.785217	14.270810	-0.058785	4.813352
289.398242	7983.985939	14.275815	-0.058776	4.811364
289.247349	7976.635695	14.280819	-0.058743	4.809214
289.363915	7969.075896	14.285824	-0.058760	4.807001
289.094279	7961.182451	14.290829	-0.058704	4.804691
289.194961	7953.392972	14.295834	-0.058718	4.802409
289.058290	7945.392320	14.300839	-0.058687	4.800065
288.917520	7937.455176	14.305843	-0.058656	4.797738
289.069092	7929.467172	14.310848	-0.058679	4.795393
288.974556	7921.412039	14.315853	-0.058656	4.793029
288.766691	7913.415436	14.320858	-0.058612	4.790682
288.828535	7905.434551	14.325863	-0.058618	4.788337
288.951285	7897.365079	14.330867	-0.058636	4.785964
288.787502	7889.401266	14.335872	-0.058600	4.783623
288.674933	7881.400837	14.340877	-0.058574	4.781269
288.679505	7873.443272	14.345882	-0.058569	4.778926
288.561590	7865.450705	14.350887	-0.058542	4.776572
288.596966	7857.344700	14.355891	-0.058543	4.774183
288.601997	7849.368282	14.360896	-0.058539	4.771832
288.777272	7841.314646	14.365901	-0.058566	4.769455
288.541087	7833.355407	14.370906	-0.058517	4.767107
288.462015	7825.365375	14.375911	-0.058497	4.764748
288.389265	7817.440703	14.380915	-0.058479	4.762407
288.459364	7809.421575	14.385920	-0.058486	4.760037
288.287722	7801.405317	14.390925	-0.058449	4.757667
288.042124	7793.365785	14.395930	-0.058398	4.755289
288.073996	7785.340288	14.400935	-0.058399	4.752913
287.868875	7777.263094	14.405939	-0.058355	4.750522
287.907872	7769.350058	14.410944	-0.058357	4.748177
287.970016	7761.328559	14.415949	-0.058364	4.745799
288.102824	7753.364539	14.420954	-0.058383	4.743436
287.836166	7745.376535	14.425959	-0.058328	4.741066
287.930233	7737.335903	14.430963	-0.058340	4.738678
288.059556	7729.372201	14.435968	-0.058359	4.736312
287.718252	7721.326231	14.440973	-0.058290	4.733922
287.831108	7713.284285	14.445978	-0.058306	4.731530
287.815968	7705.292177	14.450983	-0.058298	4.729153
287.623917	7697.335752	14.455987	-0.058257	4.726785
287.695559	7689.340071	14.460992	-0.058265	4.724403
287.711114	7681.365628	14.465997	-0.058263	4.722027
287.633559	7673.279086	14.471002	-0.058243	4.719617
287.382137	7665.346712	14.476007	-0.058191	4.717252
287.446677	7657.299144	14.481011	-0.058198	4.714850
287.442986	7649.314592	14.486016	-0.058192	4.712466
287.187228	7641.296198	14.491021	-0.058139	4.710071
287.185141	7633.346981	14.496026	-0.058133	4.707695
287.139185	7625.289707	14.501031	-0.058119	4.705286
287.237758	7617.339055	14.506035	-0.058133	4.702907
287.223173	7609.345542	14.511040	-0.058125	4.700514
286.829461	7601.355005	14.516045	-0.058046	4.698122
287.057018	7593.334227	14.521050	-0.058083	4.695718
287.098098	7585.320143	14.526055	-0.058085	4.693316
286.860374	7577.246579	14.531059	-0.058036	4.690895
286.888011	7569.300995	14.536064	-0.058036	4.688510
286.627654	7561.256476	14.541069	-0.057982	4.686095
286.729677	7553.270787	14.546074	-0.057996	4.683696
286.813434	7545.368990	14.551079	-0.058006	4.681321
286.704548	7537.312098	14.556083	-0.057981	4.678898
286.514389	7529.331503	14.561088	-0.057940	4.676497
286.511463	7521.195594	14.566093	-0.057934	4.674048
286.596417	7513.116323	14.571098	-0.057945	4.671614
286.415442	7505.236412	14.576103	-0.057906	4.669240
286.463909	7497.177671	14.581107	-0.057909	4.666810
286.486301	7489.240919	14.586112	-0.057908	4.664416
286.446312	7481.297560	14.591117	-0.057896	4.662019
286.436683	7473.235473	14.596122	-0.057889	4.659584
286.465394	7465.282146	14.601127	-0.057889	4.657181
286.352458	7457.214520	14.606131	-0.057862	4.654742
286.182005	7449.285060	14.611136	-0.057825	4.652344
286.264544	7441.177310	14.616141	-0.057836	4.649891
286.380404	7433.220345	14.621146	-0.057852	4.647482
286.320378	7425.230683	14.626151	-0.057835	4.645061
285.959829	7417.286259	14.631155	-0.057763	4.642654
285.899548	7409.242239	14.636160	-0.057747	4.640215
286.089910	7401.227028	14.641165	-0.057777	4.637783
285.817952	7393.211327	14.646170	-0.057721	4.635350
285.946835	7385.231011	14.651175	-0.057740	4.632926
286.036578	7377.168438	14.656179	-0.057751	4.630476
286.015430	7369.201165	14.661184	-0.057742	4.628053
285.885640	7361.143408	14.666189	-0.057712	4.625602
285.980580	7353.182805	14.671194	-0.057725	4.623179
285.894542	7345.237229	14.676199	-0.057704	4.620760
285.793771	7337.182120	14.681203	-0.057679	4.618306
286.106992	7329.215008	14.686208	-0.057733	4.615877
285.974405	7321.147917	14.691213	-0.057703	4.613416
285.698508	7313.164766	14.696218	-0.057646	4.610980
285.669819	7305.173979	14.701223	-0.057635	4.608540
285.591479	7297.154700	14.706227	-0.057616	4.606090
285.694487	7289.186843	14.711232	-0.057629	4.603655
285.407316	7281.191298	14.716237	-0.057571	4.601210
285.411756	7273.211463	14.721242	-0.057566	4.598768
285.482559	7265.208361	14.726247	-0.057574	4.596318
285.236569	7257.153459	14.731251	-0.057523	4.593851
285.379267	7249.133473	14.736256	-0.057544	4.591393
285.109795	7241.126031	14.741261	-0.057489	4.588937
285.024266	7233.147299	14.746266	-0.057468	4.586489
285.166582	7225.139142	14.751271	-0.057489	4.584031
284.907066	7217.153912	14.756275	-0.057435	4.581578
284.831755	7209.234809	14.761280	-0.057416	4.579145
284.884167	7201.149243	14.766285	-0.057421	4.576659
285.118896	7193.077921	14.771290	-0.057459	4.574176
285.059405	7185.114841	14.776295	-0.057443	4.571725
285.019716	7177.093189	14.781299	-0.057430	4.569254
284.805674	7169.147176	14.786304	-0.057385	4.566806
285.008979	7161.109383	14.791309	-0.057418	4.564328
284.687296	7153.161189	14.796314	-0.057352	4.561876
284.672188	7145.159938	14.801319	-0.057344	4.559406
284.664892	7137.187271	14.806323	-0.057338	4.556944
284.674654	7129.161292	14.811328	-0.057334	4.554464
284.311773	7121.119718	14.816333	-0.057262	4.551978
284.219206	7113.085780	14.821338	-0.057239	4.549493
284.354303	7105.149225	14.826343	-0.057259	4.547037
284.178623	7097.096161	14.831347	-0.057221	4.544543
284.465510	7089.197822	14.836352	-0.057269	4.542096
284.392056	7081.114881	14.841357	-0.057250	4.539591
284.260944	7073.165506	14.846362	-0.057221	4.537125
284.291988	7065.122196	14.851367	-0.057221	4.534629
284.345514	7057.122404	14.856371	-0.057226	4.532145
284.067002	7049.100537	14.861376	-0.057169	4.529652
283.959218	7041.147571	14.866381	-0.057143	4.527180
283.975772	7033.074888	14.871386	-0.057141	4.524669
284.028544	7025.201061	14.876391	-0.057146	4.522219
283.932218	7017.095786	14.881395	-0.057122	4.519695
284.024714	7009.197324	14.886400	-0.057134	4.517235
283.721324	7001.142390	14.891405	-0.057073	4.514723
283.869990	6993.034118	14.896410	-0.057095	4.512195
283.963562	6985.022724	14.901415	-0.057107	4.509695
283.885396	6977.035908	14.906419	-0.057087	4.507201
283.996536	6969.080198	14.911424	-0.057103	4.504716
283.824565	6961.112911	14.916429	-0.057066	4.502225
283.811478	6953.043147	14.921434	-0.057058	4.499702
283.678957	6945.129442	14.926439	-0.057028	4.497225
283.500697	6937.035098	14.931443	-0.056989	4.494690
283.652792	6929.077257	14.936448	-0.057013	4.492198
283.632682	6921.030597	14.941453	-0.057004	4.489675
283.385162	6913.098856	14.946458	-0.056952	4.487187
283.338709	6905.093309	14.951463	-0.056938	4.484675
283.371813	6897.082631	14.956467	-0.056939	4.482160
283.243371	6889.088822	14.961472	-0.056910	4.479648
283.165246	6881.083208	14.966477	-0.056890	4.477131
283.249608	6873.030994	14.971482	-0.056901	4.474599
283.169063	6865.065226	14.976487	-0.056880	4.472092
283.100381	6857.018602	14.981491	-0.056862	4.469558
283.217495	6849.040114	14.986496	-0.056879	4.467045
283.157267	6841.018370	14.991501	-0.056862	4.464516
283.166964	6833.070740	14.996506	-0.056859	4.462010
283.040737	6825.080551	15.001511	-0.056830	4.459488
283.099620	6817.062312	15.006515	-0.056836	4.456956
283.010688	6809.045289	15.011520	-0.056814	4.454423
282.806089	6801.021322	15.016525	-0.056771	4.451886
282.690149	6793.010883	15.021530	-0.056744	4.449352
282.820091	6785.057459	15.026535	-0.056763	4.446835
282.534000	6777.022686	15.031539	-0.056704	4.444290
282.451684	6769.069018	15.036544	-0.056684	4.441769
282.377481	6761.043016	15.041549	-0.056665	4.439224
282.348913	6753.025030	15.046554	-0.056654	4.436681
282.487877	6745.016452	15.051559	-0.056675	4.434140
282.348222	6736.925536	15.056563	-0.056643	4.431570
282.641139	6729.018464	15.061568	-0.056693	4.429058
282.391301	6720.962853	15.066573	-0.056641	4.426496
282.307958	6713.025574	15.071578	-0.056620	4.423971
282.351421	6705.011739	15.076583	-0.056623	4.421420
282.213862	6696.980492	15.081587	-0.056592	4.418861
282.224179	6688.983252	15.086592	-0.056589	4.416313
282.361487	6680.998636	15.091597	-0.056609	4.413768
282.256697	6672.961376	15.096602	-0.056584	4.411203
282.262769	6665.009366	15.101607	-0.056580	4.408664
282.033297	6656.988197	15.106611	-0.056532	4.406101
282.093136	6649.011448	15.111616	-0.056538	4.403552
281.857219	6641.020324	15.116621	-0.056489	4.400995
281.714126	6633.020828	15.121626	-0.056457	4.398435
281.918152	6625.031426	15.126631	-0.056490	4.395878
281.742202	6616.943414	15.131635	-0.056452	4.393286
281.736482	6608.969538	15.136640	-0.056445	4.390730
281.674112	6600.968136	15.141645	-0.056428	4.388164
281.678816	6592.957718	15.146650	-0.056424	4.385593
281.548206	6585.044617	15.151655	-0.056394	4.383051
281.374392	6576.982427	15.156659	-0.056357	4.380460
281.817093	6569.020559	15.161664	-0.056434	4.377903
281.684022	6561.002121	15.166669	-0.056404	4.375323
281.503038	6553.012570	15.171674	-0.056365	4.372750
281.363494	6544.979595	15.176679	-0.056334	4.370163
281.326328	6537.015504	15.181683	-0.056322	4.367596
281.272112	6529.027382	15.186688	-0.056306	4.365020
281.363676	6521.043322	15.191693	-0.056318	4.362445
281.282617	6512.962665	15.196698	-0.056298	4.359836
281.149260	6505.048242	15.201703	-0.056268	4.357278
281.094756	6497.015389	15.206707	-0.056252	4.354682
281.323849	6488.870093	15.211712	-0.056289	4.352049
281.054314	6480.873151	15.216717	-0.056234	4.349460
280.998647	6472.903022	15.221722	-0.056218	4.346879
281.000964	6464.968327	15.226727	-0.056214	4.344308
280.979259	6456.995479	15.231731	-0.056204	4.341723
280.717850	6448.989784	15.236736	-0.056150	4.339125
280.705260	6440.980198	15.241741	-0.056143	4.336525
280.671830	6432.951821	15.246746	-0.056131	4.333918
280.626724	6424.958309	15.251751	-0.056118	4.331320
280.661066	6416.938234	15.256755	-0.056119	4.328712
280.585370	6408.994332	15.261760	-0.056099	4.326127
280.342485	6400.958044	15.266765	-0.056049	4.323510
280.398383	6392.976959	15.271770	-0.056054	4.320910
280.317848	6384.971009	15.276775	-0.056034	4.318300
280.290368	6376.971671	15.281779	-0.056023	4.315691
280.250605	6368.978412	15.286784	-0.056011	4.313082
280.213998	6360.922082	15.291789	-0.055999	4.310451
280.085483	6352.949139	15.296794	-0.055970	4.307846
280.355342	6344.915890	15.301799	-0.056015	4.305221
280.096684	6336.969906	15.306803	-0.055961	4.302620
280.172986	6328.952602	15.311808	-0.055970	4.299996
280.283645	6320.954631	15.316813	-0.055985	4.297377
280.074606	6312.904105	15.321818	-0.055941	4.294737
280.144648	6304.931132	15.326823	-0.055949	4.292123
280.012570	6296.913515	15.331827	-0.055919	4.289492
279.955538	6288.958994	15.336832	-0.055903	4.286879
279.855730	6280.958122	15.341837	-0.055879	4.284250
279.916562	6272.959302	15.346842	-0.055886	4.281621
279.811017	6264.973202	15.351847	-0.055861	4.278993
279.660805	6256.934358	15.356851	-0.055827	4.276346
279.809259	6248.961443	15.361856	-0.055850	4.273721
279.617862	6240.885314	15.366861	-0.055809	4.271058
279.580295	6232.878608	15.371866	-0.055797	4.268418
279.634950	6224.885908	15.376871	-0.055801	4.265781
279.425949	6216.906718	15.381875	-0.055757	4.263145
279.439649	6208.968427	15.386880	-0.055755	4.260522
279.264146	6200.924721	15.391885	-0.055717	4.257862
279.376721	6192.933365	15.396890	-0.055732	4.255219
279.549650	6184.951015	15.401895	-0.055759	4.252579
279.369559	6176.900880	15.406899	-0.055721	4.249911
279.228694	6168.946190	15.411904	-0.055689	4.247273
279.090301	6160.921147	15.416909	-0.055658	4.244611
279.029568	6152.953664	15.421914	-0.055641	4.241967
278.968213	6144.984619	15.426919	-0.055625	4.239320
279.011955	6136.943499	15.431923	-0.055628	4.236649
279.101540	6128.955934	15.436928	-0.055639	4.233994
279.121905	6120.909595	15.441933	-0.055638	4.231318
278.911576	6112.935733	15.446938	-0.055593	4.228662
279.000395	6104.927642	15.451943	-0.055604	4.225995
278.711490	6096.940889	15.456947	-0.055545	4.223330
278.818551	6088.945208	15.461952	-0.055560	4.220665
278.682703	6081.001730	15.466957	-0.055530	4.218013
278.720267	6072.944272	15.471962	-0.055531	4.215322
278.537630	6064.962807	15.476967	-0.055492	4.212654
278.404857	6056.888876	15.481971	-0.055462	4.209953
278.421716	6048.953839	15.486976	-0.055460	4.207298
278.439901	6040.946394	15.491981	-0.055458	4.204618
278.332658	6032.996249	15.496986	-0.055433	4.201953
278.367003	6024.960352	15.501991	-0.055434	4.199260
278.325907	6016.951427	15.506995	-0.055421	4.196573
278.149437	6008.922023	15.512000	-0.055383	4.193876
278.116419	6000.835853	15.517005	-0.055371	4.191160
278.027802	5992.848599	15.522010	-0.055350	4.188475
277.903783	5984.901021	15.527015	-0.055321	4.185801
277.738301	5976.920921	15.532019	-0.055285	4.183114
277.771101	5968.929596	15.537024	-0.055286	4.180423
277.561503	5960.971455	15.542029	-0.055242	4.177740
277.630710	5952.885609	15.547034	-0.055249	4.175014
277.809247	5944.940281	15.552039	-0.055277	4.172336
277.641488	5936.847516	15.557043	-0.055241	4.169602
277.464011	5928.903649	15.562048	-0.055203	4.166916
277.482251	5920.903205	15.567053	-0.055201	4.164212
277.651453	5912.938069	15.572058	-0.055227	4.161519
277.642851	5904.919348	15.577063	-0.055220	4.158805
277.477217	5896.945180	15.582067	-0.055184	4.156102
277.425789	5888.894189	15.587072	-0.055169	4.153373
277.457816	5880.877005	15.592077	-0.055170	4.150655
277.142486	5872.909909	15.597082	-0.055106	4.147947
277.457101	5864.896421	15.602087	-0.055159	4.145229
277.439690	5856.916863	15.607091	-0.055151	4.142518
277.173449	5848.907040	15.612096	-0.055096	4.139791
277.320488	5840.934190	15.617101	-0.055118	4.137080
277.111162	5832.890903	15.622106	-0.055074	4.134339
277.107591	5824.894403	15.627111	-0.055068	4.131614
277.087821	5816.892771	15.632115	-0.055059	4.128886
276.999949	5808.917146	15.637120	-0.055037	4.126164
276.903270	5800.935257	15.642125	-0.055014	4.123438
277.003102	5792.886809	15.647130	-0.055027	4.120689
277.100270	5784.963391	15.652135	-0.055040	4.117982
276.919347	5776.896445	15.657139	-0.055001	4.115220
276.858601	5768.857985	15.662144	-0.054985	4.112468
276.787247	5760.863594	15.667149	-0.054966	4.109729
276.730565	5752.876764	15.672154	-0.054950	4.106990
276.942304	5744.891755	15.677159	-0.054985	4.104254
276.805822	5736.919454	15.682163	-0.054954	4.101516
276.609204	5728.912982	15.687168	-0.054912	4.098764
276.580122	5720.914779	15.692173	-0.054901	4.096014
276.381411	5712.907485	15.697178	-0.054859	4.093258
276.659892	5704.925688	15.702183	-0.054906	4.090515
276.428580	5696.921422	15.707187	-0.054857	4.087755
276.403324	5688.922930	15.712192	-0.054847	4.084998
276.354774	5680.977812	15.717197	-0.054833	4.082258
276.121662	5672.941186	15.722202	-0.054784	4.079482
276.071446	5665.030463	15.727207	-0.054770	4.076749
276.010951	5656.950257	15.732211	-0.054753	4.073956
275.774288	5648.940302	15.737216	-0.054704	4.071183
276.071729	5640.893198	15.742221	-0.054754	4.068403
276.048527	5632.876807	15.747226	-0.054744	4.065627
276.236130	5624.961094	15.752231	-0.054774	4.062887
276.007864	5616.932280	15.757235	-0.054726	4.060100
276.087487	5608.976753	15.762240	-0.054736	4.057340
276.129004	5600.949950	15.767245	-0.054738	4.054554
275.867335	5592.943663	15.772250	-0.054684	4.051769
275.779020	5584.960160	15.777255	-0.054663	4.048992
275.545843	5576.949547	15.782259	-0.054614	4.046201
275.629931	5568.968247	15.787264	-0.054625	4.043423
275.562657	5561.005834	15.792269	-0.054607	4.040648
275.504317	5552.953671	15.797274	-0.054591	4.037840
275.713200	5544.938913	15.802279	-0.054624	4.035047
275.588870	5536.825618	15.807283	-0.054596	4.032212
275.448766	5528.855423	15.812288	-0.054564	4.029426
275.422395	5520.898486	15.817293	-0.054554	4.026643
275.383549	5512.890509	15.822298	-0.054542	4.023841
275.138621	5504.988760	15.827303	-0.054491	4.021071
275.107724	5496.970243	15.832307	-0.054480	4.018261
275.287231	5488.934924	15.837312	-0.054508	4.015447
275.075414	5480.937254	15.842317	-0.054463	4.012637
275.119855	5472.883456	15.847322	-0.054466	4.009810
275.107716	5464.962161	15.852327	-0.054459	4.007027
274.917453	5456.929047	15.857331	-0.054418	4.004200
274.996123	5448.968772	15.862336	-0.054428	4.001400
274.891283	5440.930876	15.867341	-0.054403	3.998569
275.078670	5432.927348	15.872346	-0.054432	3.995752
274.899146	5424.939602	15.877351	-0.054394	3.992933
274.745835	5416.910408	15.882355	-0.054360	3.990097
274.805808	5408.940130	15.887360	-0.054366	3.987284
274.781809	5400.934216	15.892365	-0.054356	3.984455
274.750048	5392.967899	15.897370	-0.054345	3.981637
274.750693	5384.964306	15.902375	-0.054340	3.978805
274.773672	5376.949529	15.907379	-0.054339	3.975968
274.796610	5368.946638	15.912384	-0.054338	3.973132
274.773485	5360.930467	15.917389	-0.054328	3.970290
274.409266	5352.957012	15.922394	-0.054255	3.967454
274.474859	5344.990454	15.927399	-0.054262	3.964626
274.310008	5337.024550	15.932403	-0.054226	3.961793
274.477162	5329.023350	15.937408	-0.054252	3.958950
274.223994	5321.043307	15.942413	-0.054200	3.956106
273.970790	5312.976230	15.947418	-0.054147	3.953229
274.022339	5304.942655	15.952423	-0.054152	3.950366
274.100815	5296.917975	15.957427	-0.054161	3.947506
274.013467	5288.949897	15.962432	-0.054139	3.944660
273.939693	5281.018414	15.967437	-0.054120	3.941826
273.882165	5272.980997	15.972442	-0.054104	3.938952
274.006301	5265.017427	15.977447	-0.054122	3.936106
273.869401	5256.985125	15.982451	-0.054092	3.933229
273.887377	5248.985155	15.987456	-0.054090	3.930363
273.812676	5241.033885	15.992461	-0.054071	3.927512
273.584543	5233.004661	15.997466	-0.054023	3.924627
273.615042	5225.049466	16.002471	-0.054023	3.921772
273.682870	5216.990483	16.007475	-0.054031	3.918878
273.812294	5209.005532	16.012480	-0.054049	3.916009
273.574039	5201.001463	16.017485	-0.054000	3.913125
273.562454	5192.959049	16.022490	-0.053992	3.910229
273.605269	5185.010797	16.027495	-0.053995	3.907366
273.348199	5177.000496	16.032499	-0.053942	3.904473
273.446594	5169.025701	16.037504	-0.053955	3.901597
273.463802	5161.028066	16.042509	-0.053953	3.898709
273.328054	5153.003622	16.047514	-0.053922	3.895806
273.305385	5145.021679	16.052519	-0.053913	3.892919
273.105808	5136.984983	16.057523	-0.053871	3.890007
273.078509	5129.016105	16.062528	-0.053860	3.887120
273.176881	5121.018202	16.067533	-0.053873	3.884222
273.173652	5113.021223	16.072538	-0.053867	3.881322
273.202700	5105.046590	16.077543	-0.053868	3.878427
272.889302	5097.014347	16.082547	-0.053804	3.875503
272.941623	5088.827327	16.087552	-0.053808	3.872527
272.857383	5080.832242	16.092557	-0.053787	3.869617
272.780025	5072.913985	16.097562	-0.053768	3.866732
272.777789	5064.970253	16.102567	-0.053762	3.863837
272.620219	5056.952676	16.107571	-0.053728	3.860910
272.525722	5049.006265	16.112576	-0.053705	3.858009
272.492439	5040.988229	16.117581	-0.053693	3.855080
272.396980	5032.971999	16.122586	-0.053670	3.852148
272.447366	5025.023936	16.127591	-0.053674	3.849241
272.399482	5017.015621	16.132595	-0.053660	3.846309
272.299759	5009.042692	16.137600	-0.053636	3.843386
272.229164	5001.048738	16.142605	-0.053618	3.840454
272.100830	4993.053910	16.147610	-0.053589	3.837518
272.179717	4985.069071	16.152615	-0.053598	3.834588
272.255706	4977.006391	16.157619	-0.053607	3.831626
272.337687	4969.013230	16.162624	-0.053617	3.828689
272.116615	4961.047397	16.167629	-0.053571	3.825752
271.885784	4953.055284	16.172634	-0.053522	3.822804
271.971357	4945.091385	16.177639	-0.053533	3.819870
271.918254	4937.084743	16.182643	-0.053518	3.816916
271.772783	4929.128465	16.187648	-0.053486	3.813975
271.844100	4921.083253	16.192653	-0.053494	3.811004
271.745762	4913.103793	16.197658	-0.053470	3.808052
271.716118	4905.108918	16.202663	-0.053459	3.805093
271.774169	4897.141355	16.207667	-0.053465	3.802143
271.525750	4889.129459	16.212672	-0.053413	3.799169
271.467912	4881.150765	16.217677	-0.053397	3.796208
271.396186	4873.068159	16.222682	-0.053379	3.793206
271.666395	4865.077036	16.227687	-0.053424	3.790244
271.470930	4857.070640	16.232691	-0.053382	3.787263
271.495249	4849.092112	16.237696	-0.053381	3.784295
271.523821	4841.111209	16.242701	-0.053381	3.781323
271.386363	4833.088611	16.247706	-0.053351	3.778331
271.358640	4825.121150	16.252711	-0.053340	3.775359
271.017572	4817.120114	16.257715	-0.053271	3.772365
271.156754	4809.079350	16.262720	-0.053292	3.769364
271.100018	4801.145163	16.267725	-0.053276	3.766397
270.826523	4793.141879	16.272730	-0.053220	3.763396
270.878713	4785.164628	16.277735	-0.053225	3.760410
270.637071	4777.199822	16.282739	-0.053174	3.757420
270.688486	4769.137136	16.287744	-0.053179	3.754397
270.699502	4761.149903	16.292749	-0.053175	3.751399
270.809979	4753.091533	16.297754	-0.053191	3.748375
270.755291	4745.111176	16.302759	-0.053175	3.745373
270.495426	4737.165625	16.307763	-0.053122	3.742378
270.606986	4729.119937	16.312768	-0.053137	3.739351
270.544634	4721.188371	16.317773	-0.053120	3.736360
270.471421	4713.148852	16.322778	-0.053101	3.733326
270.426803	4705.113299	16.327783	-0.053088	3.730292
270.351310	4697.163890	16.332787	-0.053068	3.727287
270.489801	4689.155522	16.337792	-0.053089	3.724262
270.621560	4681.184543	16.342797	-0.053108	3.721249
270.323422	4673.193511	16.347802	-0.053048	3.718216
270.253212	4665.239185	16.352807	-0.053029	3.715199
270.375241	4657.106391	16.357811	-0.053047	3.712117
270.413903	4649.124531	16.362816	-0.053049	3.709088
270.322171	4641.173933	16.367821	-0.053026	3.706065
270.139241	4633.193853	16.372826	-0.052987	3.703026
270.220717	4625.195229	16.377831	-0.052997	3.699984
270.003772	4617.240404	16.382835	-0.052951	3.696949
270.045331	4609.201832	16.387840	-0.052954	3.693886
269.842115	4601.231587	16.392845	-0.052911	3.690840
269.786768	4593.222444	16.397850	-0.052895	3.687780
269.990777	4585.215317	16.402855	-0.052928	3.684725
269.780457	4577.261425	16.407859	-0.052883	3.681678
269.741711	4569.254864	16.412864	-0.052871	3.678612
269.705493	4561.274385	16.417869	-0.052859	3.675554
269.622073	4553.239387	16.422874	-0.052838	3.672471
269.658843	4545.236567	16.427879	-0.052840	3.669401
269.610678	4537.263949	16.432883	-0.052825	3.666337
269.487598	4529.257544	16.437888	-0.052797	3.663256
269.236000	4521.270573	16.442893	-0.052745	3.660177
269.345182	4513.267905	16.447898	-0.052760	3.657099
269.282646	4505.254312	16.452903	-0.052743	3.654009
269.018052	4497.253050	16.457907	-0.052689	3.650916
269.211138	4489.282750	16.462912	-0.052720	3.647844
268.964224	4481.289925	16.467917	-0.052668	3.644750
268.965048	4473.325106	16.472922	-0.052663	3.641670
268.982270	4465.338497	16.477927	-0.052661	3.638579
268.879568	4457.318526	16.482931	-0.052637	3.635470
268.709123	4449.281937	16.487936	-0.052600	3.632350
268.894641	4441.280957	16.492941	-0.052629	3.629250
268.881664	4433.254610	16.497946	-0.052621	3.626133
268.895329	4425.281509	16.502951	-0.052619	3.623034
268.782355	4417.291916	16.507955	-0.052592	3.619923
268.667526	4409.331019	16.512960	-0.052566	3.616821
268.750635	4401.299951	16.517965	-0.052576	3.613693
268.463562	4393.291273	16.522970	-0.052517	3.610562
268.450801	4385.345600	16.527975	-0.052510	3.607460
268.450357	4377.316449	16.532979	-0.052504	3.604323
268.497085	4369.380351	16.537984	-0.052508	3.601221
268.419388	4361.431961	16.542989	-0.052488	3.598108
268.207679	4353.395623	16.547994	-0.052443	3.594954
268.227111	4345.406529	16.552999	-0.052442	3.591823
268.140417	4337.378679	16.558003	-0.052420	3.588670
268.392804	4329.367075	16.563008	-0.052462	3.585530
268.185736	4321.457216	16.568013	-0.052418	3.582415
267.947287	4313.418579	16.573018	-0.052369	3.579246
268.126172	4305.433985	16.578023	-0.052397	3.576107
267.795715	4297.440065	16.583027	-0.052330	3.572947
267.778418	4289.420411	16.588032	-0.052321	3.569782
267.890949	4281.449037	16.593037	-0.052337	3.566638
267.592436	4273.452981	16.598042	-0.052276	3.563470
267.655838	4265.483516	16.603047	-0.052283	3.560319
267.725736	4257.484347	16.608051	-0.052291	3.557155
267.619335	4249.435906	16.613056	-0.052265	3.553962
267.476406	4241.359672	16.618061	-0.052234	3.550755
267.275793	4233.394113	16.623066	-0.052191	3.547587
267.257505	4225.418350	16.628071	-0.052182	3.544418
267.251059	4217.434733	16.633075	-0.052176	3.541243
267.032782	4209.493638	16.638080	-0.052130	3.538075
266.996097	4201.481988	16.643085	-0.052118	3.534883
267.009804	4193.429225	16.648090	-0.052115	3.531672
267.003243	4185.471309	16.653095	-0.052109	3.528496
267.092978	4177.463336	16.658099	-0.052120	3.525299
266.727757	4169.514040	16.663104	-0.052047	3.522110
266.983237	4161.501835	16.668109	-0.052089	3.518911
266.736002	4153.518519	16.673114	-0.052038	3.515706
266.657314	4145.531361	16.678119	-0.052018	3.512501
266.607540	4137.516673	16.683123	-0.052003	3.509283
266.533196	4129.538432	16.688128	-0.051984	3.506076
266.253835	4121.601846	16.693133	-0.051927	3.502877
266.258177	4113.537663	16.698138	-0.051923	3.499632
266.427087	4105.588392	16.703143	-0.051949	3.496435
266.417792	4097.543179	16.708147	-0.051942	3.493191
266.540765	4089.507598	16.713152	-0.051959	3.489953
266.212861	4081.644934	16.718157	-0.051893	3.486767
266.263066	4073.546425	16.723162	-0.051897	3.483494
266.228421	4065.625603	16.728167	-0.051886	3.480288
266.408676	4057.623671	16.733171	-0.051914	3.477052
266.181202	4049.615608	16.738176	-0.051866	3.473799
266.204263	4041.592424	16.743181	-0.051865	3.470544
266.059939	4033.585319	16.748186	-0.051833	3.467287
266.223201	4025.610679	16.753191	-0.051858	3.464050
265.679055	4017.658701	16.758195	-0.051752	3.460796
265.788965	4009.642708	16.763200	-0.051767	3.457535
266.000723	4001.652165	16.768205	-0.051801	3.454284
265.815808	3993.618057	16.773210	-0.051761	3.450999
265.747108	3985.666445	16.778215	-0.051743	3.447749
265.637835	3977.622582	16.783219	-0.051718	3.444457
265.940540	3969.658639	16.788224	-0.051769	3.441207
265.954856	3961.678806	16.793229	-0.051766	3.437939
265.635110	3953.686305	16.798234	-0.051702	3.434651
265.651565	3945.686610	16.803239	-0.051699	3.431368
265.672493	3937.651669	16.808243	-0.051698	3.428068
265.646676	3929.656333	16.813248	-0.051688	3.424779
265.700134	3921.750942	16.818253	-0.051693	3.421527
265.610938	3913.734414	16.823258	-0.051671	3.418221
265.498574	3905.765416	16.828263	-0.051645	3.414931
265.473542	3897.725185	16.833267	-0.051635	3.411611
265.320505	3889.752402	16.838272	-0.051601	3.408311
265.468917	3881.746744	16.843277	-0.051623	3.405005
265.188760	3873.812820	16.848282	-0.051566	3.401711
265.382760	3865.806067	16.853287	-0.051597	3.398399
265.330396	3857.805652	16.858291	-0.051582	3.395079
265.026063	3849.750627	16.863296	-0.051520	3.391723
265.204525	3841.737059	16.868301	-0.051548	3.388399
265.101492	3833.751792	16.873306	-0.051523	3.385073
265.017522	3825.829025	16.878311	-0.051503	3.381770
264.480682	3817.870458	16.883315	-0.051397	3.378434
264.678613	3809.841003	16.888320	-0.051429	3.375090
264.733080	3801.849442	16.893325	-0.051434	3.371754
264.737280	3793.833448	16.898330	-0.051429	3.368403
264.946244	3785.832695	16.903335	-0.051463	3.365062
264.704154	3777.913839	16.908339	-0.051413	3.361735
264.514548	3769.902486	16.913344	-0.051372	3.358369
264.383839	3761.927688	16.918349	-0.051343	3.355016
264.376971	3753.862716	16.923354	-0.051336	3.351627
264.398804	3745.898406	16.928359	-0.051335	3.348278
264.356688	3737.874182	16.933363	-0.051322	3.344898
264.195844	3729.931242	16.938368	-0.051286	3.341544
264.461885	3721.910719	16.943373	-0.051331	3.338170
263.874633	3713.954225	16.948378	-0.051216	3.334788
264.063629	3705.962442	16.953383	-0.051246	3.331416
264.074334	3697.944008	16.958387	-0.051243	3.328023
264.006360	3689.927342	16.963392	-0.051225	3.324625
264.125917	3681.984227	16.968397	-0.051242	3.321261
264.157664	3673.979601	16.973402	-0.051243	3.317864
264.008301	3666.035014	16.978407	-0.051210	3.314483
263.641474	3658.035547	16.983411	-0.051136	3.311066
263.625246	3650.017323	16.988416	-0.051128	3.307651
263.687347	3642.030496	16.993421	-0.051134	3.304249
263.550377	3634.025590	16.998426	-0.051103	3.300828
263.937190	3626.035975	17.003431	-0.051170	3.297430
263.919996	3618.039202	17.008435	-0.051162	3.294011
263.754878	3610.037665	17.013440	-0.051126	3.290580
263.614132	3602.086081	17.018445	-0.051094	3.287167
263.712260	3594.060363	17.023450	-0.051107	3.283729
263.545710	3586.116137	17.028455	-0.051071	3.280311
263.453564	3578.171416	17.033459	-0.051048	3.276893
263.419613	3570.134794	17.038464	-0.051037	3.273434
263.502689	3562.105554	17.043469	-0.051047	3.269979
263.337023	3554.155727	17.048474	-0.051011	3.266545
263.317134	3546.165720	17.053479	-0.051002	3.263095
263.138982	3538.182651	17.058483	-0.050964	3.259639
263.059059	3530.211470	17.063488	-0.050943	3.256188
262.953553	3522.214362	17.068493	-0.050919	3.252721
262.996804	3514.171219	17.073498	-0.050921	3.249236
263.168230	3506.191830	17.078503	-0.050948	3.245780
262.827956	3498.248399	17.083507	-0.050879	3.242316
262.840581	3490.250335	17.088512	-0.050877	3.238838
262.891697	3482.273084	17.093517	-0.050881	3.235368
262.701604	3474.206349	17.098522	-0.050840	3.231844
262.806763	3466.207737	17.103527	-0.050854	3.228359
262.879836	3458.199972	17.108531	-0.050863	3.224865
262.600841	3450.278518	17.113536	-0.050806	3.221390
262.667664	3442.297203	17.118541	-0.050813	3.217899
262.640238	3434.274919	17.123546	-0.050802	3.214383
262.692200	3426.280329	17.128551	-0.050807	3.210878
262.610759	3418.316178	17.133555	-0.050786	3.207377
262.401411	3410.331605	17.138560	-0.050742	3.203858
262.366825	3402.386266	17.143565	-0.050731	3.200360
262.172117	3394.403113	17.148570	-0.050689	3.196835
262.095553	3386.407803	17.153575	-0.050670	3.193305
262.111105	3378.374498	17.158579	-0.050667	3.189759
262.060783	3370.381782	17.163584	-0.050653	3.186223
261.943482	3362.423367	17.168589	-0.050625	3.182696
261.789936	3354.446298	17.173594	-0.050592	3.179156
261.887487	3346.458457	17.178599	-0.050605	3.175617
261.804190	3338.440549	17.183603	-0.050584	3.172053
261.638275	3330.434700	17.188608	-0.050548	3.168487
261.586146	3322.486621	17.193613	-0.050533	3.164948
261.615857	3314.487063	17.198618	-0.050533	3.161385
261.565284	3306.551121	17.203623	-0.050518	3.157843
261.422917	3298.546331	17.208627	-0.050487	3.154262
261.406883	3290.472870	17.213632	-0.050478	3.150652
261.494987	3282.496873	17.218637	-0.050489	3.147086
261.687475	3274.465415	17.223642	-0.050520	3.143496
261.635773	3266.537766	17.228647	-0.050505	3.139938
261.644356	3258.579206	17.233651	-0.050501	3.136364
261.277057	3250.594980	17.238656	-0.050428	3.132758
261.526128	3242.587487	17.243661	-0.050469	3.129165
261.115417	3234.626130	17.248666	-0.050387	3.125559
261.070389	3226.647891	17.253671	-0.050374	3.121957
261.141676	3218.670876	17.258675	-0.050382	3.118357
261.124783	3210.663448	17.263680	-0.050373	3.114735
261.131955	3202.666410	17.268685	-0.050369	3.111115
260.914953	3194.675430	17.273690	-0.050324	3.107483
260.985939	3186.687306	17.278695	-0.050332	3.103861
260.939379	3178.712614	17.283699	-0.050318	3.100236
260.835558	3170.735152	17.288704	-0.050293	3.096603
260.940760	3162.739375	17.293709	-0.050307	3.092966
260.668092	3154.731921	17.298714	-0.050251	3.089303
260.711469	3146.742738	17.303719	-0.050254	3.085658
260.658424	3138.802021	17.308723	-0.050239	3.082026
260.611638	3130.831876	17.313728	-0.050225	3.078377
260.467441	3122.848341	17.318733	-0.050193	3.074713
260.511462	3114.720001	17.323738	-0.050196	3.070987
260.611017	3106.765745	17.328743	-0.050209	3.067339
260.376703	3098.810666	17.333747	-0.050160	3.063671
260.164675	3090.835858	17.338752	-0.050116	3.059990
260.355892	3082.890617	17.343757	-0.050146	3.056337
260.109427	3074.874346	17.348762	-0.050095	3.052627
260.203889	3066.900632	17.353767	-0.050107	3.048947
260.182421	3058.897780	17.358771	-0.050098	3.045245
259.993065	3050.942116	17.363776	-0.050058	3.041551
259.934408	3042.995562	17.368781	-0.050041	3.037864
259.972194	3034.986921	17.373786	-0.050043	3.034148
260.071275	3026.958254	17.378791	-0.050056	3.030421
260.003618	3018.970736	17.383795	-0.050038	3.026700
259.871081	3011.009172	17.388800	-0.050009	3.022984
259.767733	3003.069152	17.393805	-0.049984	3.019275
259.643682	2995.085657	17.398810	-0.049956	3.015540
259.697653	2987.056213	17.403815	-0.049961	3.011787
259.512925	2979.088318	17.408819	-0.049921	3.008047
259.543190	2971.095305	17.413824	-0.049921	3.004301
259.674235	2963.126280	17.418829	-0.049940	3.000566
259.458950	2955.176245	17.423834	-0.049895	2.996819
259.372991	2947.163001	17.428839	-0.049874	2.993044
259.022493	2939.183813	17.433843	-0.049803	2.989266
258.849226	2931.190237	17.438848	-0.049766	2.985486
259.213841	2923.187646	17.443853	-0.049828	2.981724
259.268686	2915.192823	17.448858	-0.049833	2.977945
259.178823	2907.224797	17.453863	-0.049811	2.974167
259.012244	2899.251416	17.458867	-0.049775	2.970377
258.971585	2891.282114	17.463872	-0.049762	2.966591
259.057256	2883.297714	17.468877	-0.049773	2.962800
258.642332	2875.357348	17.473882	-0.049691	2.958999
258.895649	2867.327032	17.478887	-0.049732	2.955184
258.706087	2859.332902	17.483891	-0.049692	2.951359
258.618186	2851.350713	17.488896	-0.049670	2.947540
258.474129	2843.424738	17.493901	-0.049638	2.943739
258.636996	2835.375682	17.498906	-0.049663	2.939891
258.513745	2827.410924	17.503911	-0.049635	2.936064
258.362402	2819.447970	17.508915	-0.049602	2.932230
258.495052	2811.424492	17.513920	-0.049621	2.928378
258.282728	2803.489150	17.518925	-0.049576	2.924545
258.037186	2795.516189	17.523930	-0.049525	2.920687
258.024073	2787.588631	17.528935	-0.049518	2.916857
258.030249	2779.494536	17.533939	-0.049514	2.912944
258.125096	2771.433184	17.538944	-0.049526	2.909045
258.010642	2763.507202	17.543949	-0.049499	2.905196
258.045085	2755.518241	17.548954	-0.049501	2.901319
258.047617	2747.581956	17.553959	-0.049496	2.897461
258.128820	2739.578995	17.558963	-0.049506	2.893569
258.099675	2731.568860	17.563968	-0.049495	2.889663
258.095341	2723.648002	17.568973	-0.049489	2.885797
257.718737	2715.710074	17.573978	-0.049414	2.881896
257.690128	2707.733633	17.578983	-0.049403	2.877991
257.943425	2699.701680	17.583987	-0.049445	2.874068
257.580014	2691.721914	17.588992	-0.049372	2.870132
257.852930	2683.743233	17.593997	-0.049418	2.866225
257.679587	2675.756061	17.599002	-0.049380	2.862285
257.527505	2667.809888	17.604007	-0.049347	2.858361
257.484156	2659.815733	17.609011	-0.049333	2.854413
257.550744	2651.796948	17.614016	-0.049340	2.850454
257.510040	2643.855562	17.619021	-0.049328	2.846522
257.408707	2635.893603	17.624026	-0.049303	2.842571
257.308161	2627.931365	17.629031	-0.049279	2.838614
257.101970	2619.995374	17.634035	-0.049236	2.834659
257.095524	2611.921923	17.639040	-0.049229	2.830641
257.061374	2603.964502	17.644045	-0.049218	2.826673
256.959996	2595.977779	17.649050	-0.049194	2.822682
257.000753	2588.003697	17.654055	-0.049196	2.818699
256.655489	2580.071197	17.659059	-0.049126	2.814710
256.492394	2572.075154	17.664064	-0.049091	2.810693
256.279055	2564.160409	17.669069	-0.049046	2.806708
256.184250	2556.122387	17.674074	-0.049023	2.802663
256.547759	2548.128901	17.679079	-0.049085	2.798660
256.417164	2540.158949	17.684083	-0.049056	2.794635
256.379341	2532.128053	17.689088	-0.049044	2.790579
256.605601	2524.156118	17.694093	-0.049080	2.786562
256.112066	2516.220264	17.699098	-0.048983	2.782516
256.051131	2508.265798	17.704103	-0.048967	2.778480
255.955747	2500.295586	17.709107	-0.048944	2.774427
256.003740	2492.244937	17.714112	-0.048947	2.770337
256.128923	2484.296410	17.719117	-0.048965	2.766296
256.042504	2476.317426	17.724122	-0.048944	2.762222
255.940255	2468.385096	17.729127	-0.048920	2.758165
256.200737	2460.358611	17.734131	-0.048963	2.754075
256.007691	2452.297186	17.739136	-0.048922	2.749934
256.031866	2444.352640	17.744141	-0.048921	2.745860
255.953139	2436.384004	17.749146	-0.048901	2.741761
256.066677	2428.416803	17.754151	-0.048917	2.737668
255.691321	2420.488870	17.759155	-0.048842	2.733560
255.655319	2412.483995	17.764160	-0.048830	2.729426
255.752403	2404.532244	17.769165	-0.048843	2.725322
255.542541	2396.574575	17.774170	-0.048799	2.721190
255.454932	2388.606166	17.779175	-0.048777	2.717053
255.503242	2380.622355	17.784179	-0.048781	2.712911
255.422232	2372.617529	17.789184	-0.048760	2.708743
255.423216	2364.651818	17.794189	-0.048755	2.704594
255.259130	2356.699523	17.799194	-0.048720	2.700435
255.420908	2348.737266	17.804199	-0.048745	2.696286
255.264113	2340.760399	17.809203	-0.048710	2.692102
255.150613	2332.778914	17.814208	-0.048684	2.687912
255.223839	2324.817184	17.819213	-0.048692	2.683737
255.100278	2316.828616	17.824218	-0.048664	2.679530
255.209528	2308.873733	17.829223	-0.048679	2.675348
255.263709	2300.859207	17.834227	-0.048684	2.671125
254.895234	2292.911462	17.839232	-0.048610	2.666904
254.918364	2284.936086	17.844237	-0.048609	2.662686
254.786285	2276.970993	17.849242	-0.048579	2.658457
254.739672	2269.018829	17.854247	-0.048565	2.654233
254.484683	2261.042540	17.859251	-0.048513	2.649977
254.592547	2253.034622	17.864256	-0.048527	2.645720
254.544990	2245.105325	17.869261	-0.048513	2.641488
254.311196	2237.151415	17.874266	-0.048465	2.637224
254.317810	2229.149237	17.879271	-0.048461	2.632944
254.392659	2221.142659	17.884275	-0.048469	2.628658
254.346558	2213.156711	17.889280	-0.048455	2.624368
254.347245	2205.223623	17.894285	-0.048450	2.620103
254.139989	2197.284804	17.899290	-0.048406	2.615814
254.018766	2189.316971	17.904295	-0.048379	2.611508
253.984090	2181.329979	17.909299	-0.048367	2.607190
253.886427	2173.352519	17.914304	-0.048343	2.602866
254.269195	2165.365519	17.919309	-0.048410	2.598562
254.009815	2157.401326	17.924314	-0.048356	2.594220
253.893788	2149.258985	17.929319	-0.048329	2.589784
254.006261	2141.318842	17.934323	-0.048345	2.585465
253.690690	2133.413391	17.939328	-0.048281	2.581129
253.733681	2125.467105	17.944333	-0.048284	2.576788
253.426568	2117.532791	17.949338	-0.048221	2.572422
253.487216	2109.556846	17.954343	-0.048227	2.568051
253.415547	2101.592631	17.959347	-0.048209	2.563670
253.353013	2093.645735	17.964352	-0.048192	2.559291
253.637221	2085.659391	17.969357	-0.048239	2.554908
253.660636	2077.662487	17.974362	-0.048239	2.550493
253.302602	2069.725711	17.979367	-0.048167	2.546076
253.458972	2061.766423	17.984371	-0.048191	2.541676
253.286931	2053.804076	17.989376	-0.048153	2.537243
253.260431	2045.839204	17.994381	-0.048143	2.532812
252.984119	2037.907213	17.999386	-0.048086	2.528373
253.070761	2029.914808	18.004391	-0.048097	2.523918
252.970415	2021.977631	18.009395	-0.048073	2.519473
253.019606	2013.988887	18.014400	-0.048077	2.515002
252.982522	2006.008967	18.019405	-0.048065	2.510522
252.877314	1998.016257	18.024410	-0.048040	2.506022
252.848609	1990.067462	18.029415	-0.048030	2.501543
252.755760	1982.129279	18.034419	-0.048007	2.497059
252.694020	1974.135168	18.039424	-0.047990	2.492536
252.708623	1966.185686	18.044429	-0.047988	2.488036
252.619149	1958.211231	18.049434	-0.047966	2.483507
252.691294	1950.266405	18.054439	-0.047974	2.478997
252.553525	1942.332517	18.059443	-0.047943	2.474471
252.252011	1934.362844	18.064448	-0.047882	2.469903
252.355000	1926.385517	18.069453	-0.047896	2.465353
252.280281	1918.439452	18.074458	-0.047877	2.460798
252.225256	1910.480551	18.079463	-0.047861	2.456230
252.168037	1902.512344	18.084467	-0.047845	2.451647
252.176456	1894.525824	18.089472	-0.047842	2.447050
251.990605	1886.601924	18.094477	-0.047802	2.442466
251.894211	1878.635929	18.099482	-0.047779	2.437856
251.992769	1870.621995	18.104487	-0.047792	2.433224
251.958938	1862.618357	18.109491	-0.047780	2.428579
251.823367	1854.655529	18.114496	-0.047750	2.423941
251.752818	1846.745507	18.119501	-0.047731	2.419330
251.664824	1838.789818	18.124506	-0.047710	2.414682
251.415304	1830.845530	18.129511	-0.047658	2.410020
251.540192	1822.854086	18.134515	-0.047676	2.405349
251.341521	1814.940166	18.139520	-0.047634	2.400690
251.441519	1806.986634	18.144525	-0.047647	2.396022
251.174644	1799.022987	18.149530	-0.047592	2.391310
251.378578	1791.014799	18.154535	-0.047625	2.386599
251.239726	1783.091260	18.159539	-0.047594	2.381902
251.094087	1775.145390	18.164544	-0.047562	2.377182
250.972335	1767.201420	18.169549	-0.047534	2.372456
250.971057	1759.208438	18.174554	-0.047528	2.367701
250.662305	1751.315705	18.179559	-0.047466	2.362971
250.618314	1743.355580	18.184563	-0.047452	2.358212
250.625816	1735.361616	18.189568	-0.047448	2.353428
250.827906	1727.356343	18.194573	-0.047481	2.348643
250.636868	1719.402444	18.199578	-0.047440	2.343848
250.530055	1711.471672	18.204583	-0.047415	2.339063
250.523721	1703.538407	18.209587	-0.047408	2.334275
250.196913	1695.595007	18.214592	-0.047342	2.329445
250.369652	1687.622293	18.219597	-0.047369	2.324628
250.302586	1679.667788	18.224602	-0.047352	2.319792
250.285174	1671.725957	18.229607	-0.047343	2.314958
250.118391	1663.773275	18.234611	-0.047307	2.310095
250.069129	1655.799690	18.239616	-0.047292	2.305218
250.185124	1647.848907	18.244621	-0.047309	2.300360
249.988963	1639.914154	18.249626	-0.047267	2.295474
249.827932	1631.979676	18.254631	-0.047232	2.290581
250.171713	1623.964035	18.259635	-0.047291	2.285670
249.997720	1616.042937	18.264640	-0.047253	2.280763
250.013406	1608.113358	18.269645	-0.047251	2.275857
249.752954	1600.126087	18.274650	-0.047197	2.270880
249.693233	1592.146563	18.279655	-0.047181	2.265915
249.433063	1584.250841	18.284659	-0.047127	2.260973
249.345252	1576.310452	18.289664	-0.047105	2.256008
249.436651	1568.328584	18.294669	-0.047117	2.251021
249.096544	1560.419568	18.299674	-0.047049	2.246031
249.268684	1552.423327	18.304679	-0.047075	2.241020
249.403462	1544.487914	18.309683	-0.047095	2.236033
249.151313	1536.538641	18.314688	-0.047043	2.230992
249.128764	1528.597589	18.319693	-0.047034	2.225965
248.912351	1520.685381	18.324698	-0.046988	2.220928
249.115460	1512.695925	18.329703	-0.047021	2.215867
248.988318	1504.757445	18.334707	-0.046992	2.210798
248.552185	1496.880910	18.339712	-0.046906	2.205729
248.975093	1488.870719	18.344717	-0.046979	2.200640
248.982846	1480.909773	18.349722	-0.046975	2.195533
248.613433	1472.997997	18.354727	-0.046901	2.190412
248.623614	1465.031986	18.359731	-0.046898	2.185278
248.715253	1457.071457	18.364736	-0.046910	2.180144
248.554665	1449.190133	18.369741	-0.046875	2.175025
248.552402	1441.224055	18.374746	-0.046869	2.169854
248.552403	1433.262254	18.379751	-0.046864	2.164673
248.130465	1425.417288	18.384755	-0.046780	2.159517
247.958273	1417.452992	18.389760	-0.046743	2.154294
248.276796	1409.438359	18.394765	-0.046797	2.149071
248.217840	1401.502098	18.399770	-0.046781	2.143851
247.922827	1393.606171	18.404775	-0.046720	2.138623
247.964239	1385.669522	18.409779	-0.046723	2.133387
247.565599	1377.769722	18.414784	-0.046643	2.128120
247.539446	1369.817696	18.419789	-0.046633	2.122842
247.370290	1361.906952	18.424794	-0.046597	2.117564
247.154431	1353.933685	18.429799	-0.046551	2.112226
247.175802	1345.936945	18.434803	-0.046550	2.106882
247.230540	1337.987507	18.439808	-0.046555	2.101560
247.639954	1330.007795	18.444813	-0.046626	2.096238
247.558421	1322.069801	18.449818	-0.046606	2.090883
247.384895	1314.165058	18.454823	-0.046568	2.085527
247.408082	1306.270364	18.459827	-0.046567	2.080184
247.209692	1298.358768	18.464832	-0.046525	2.074794
247.120440	1290.410517	18.469837	-0.046503	2.069375
246.852863	1282.513004	18.474842	-0.046448	2.063959
247.274633	1274.520766	18.479847	-0.046521	2.058533
246.865827	1266.658806	18.484851	-0.046440	2.053099
246.730949	1258.707388	18.489856	-0.046410	2.047616
246.691053	1250.797337	18.494861	-0.046397	2.042156
246.798703	1242.850506	18.499866	-0.046412	2.036672
246.464200	1234.934846	18.504871	-0.046345	2.031149
246.641074	1226.963265	18.509875	-0.046372	2.025624
246.388101	1219.062270	18.514880	-0.046320	2.020090
246.365645	1211.147099	18.519885	-0.046311	2.014554
246.301037	1203.201421	18.524890	-0.046293	2.008977
246.641239	1195.227730	18.529895	-0.046351	2.003407
246.599625	1187.336872	18.534899	-0.046338	1.997840
246.213800	1179.443412	18.539904	-0.046261	1.992219
246.470190	1171.478276	18.544909	-0.046304	1.986600
246.471994	1163.562981	18.549914	-0.046299	1.980972
246.151982	1155.691152	18.554919	-0.046234	1.975326
246.017339	1147.785007	18.559923	-0.046204	1.969659
245.629111	1139.919539	18.564928	-0.046127	1.963977
245.954870	1131.940533	18.569933	-0.046182	1.958274
245.523818	1124.057068	18.574938	-0.046097	1.952541
245.562810	1116.063322	18.579943	-0.046099	1.946763
245.651045	1108.132049	18.584947	-0.046110	1.941018
245.544903	1100.226787	18.589952	-0.046085	1.935253
245.542533	1092.321201	18.594957	-0.046079	1.929483
245.320551	1084.428017	18.599962	-0.046033	1.923680
245.215578	1076.525669	18.604967	-0.046008	1.917866
245.276974	1068.590272	18.609971	-0.046014	1.912028
245.235515	1060.640141	18.614976	-0.046001	1.906150
245.317138	1052.726825	18.619981	-0.046011	1.900295
245.130908	1044.858884	18.624986	-0.045971	1.894425
245.141806	1036.927437	18.629991	-0.045968	1.888512
245.074777	1029.037418	18.634995	-0.045950	1.882602
244.882275	1021.149948	18.640000	-0.045909	1.876662
244.826448	1013.232813	18.645005	-0.045894	1.870696
244.820316	1005.302000	18.650010	-0.045887	1.864706
244.679575	997.423773	18.655015	-0.045856	1.858721
244.693121	989.514406	18.660019	-0.045853	1.852711
244.454565	981.626325	18.665024	-0.045804	1.846668
244.749912	973.675886	18.670029	-0.045854	1.840620
244.377152	965.844871	18.675034	-0.045779	1.834566
244.187982	957.940964	18.680039	-0.045739	1.828456
244.342394	950.017198	18.685043	-0.045762	1.822352
244.160190	942.144115	18.690048	-0.045723	1.816227
244.183226	934.225396	18.695053	-0.045722	1.810069
244.277283	926.307419	18.700058	-0.045734	1.803900
244.300090	918.424432	18.705063	-0.045733	1.797728
244.149469	910.517180	18.710067	-0.045700	1.791495
243.988178	902.604817	18.715072	-0.045665	1.785235
244.075480	894.715793	18.720077	-0.045676	1.779002
243.898510	886.844149	18.725082	-0.045638	1.772728
243.870610	878.942307	18.730087	-0.045628	1.766426
243.920487	871.064513	18.735091	-0.045632	1.760130
243.645061	863.223813	18.740096	-0.045575	1.753801
243.653903	855.303616	18.745101	-0.045572	1.747421
243.658435	847.424522	18.750106	-0.045567	1.741050
243.474242	839.565937	18.755111	-0.045528	1.734648
243.531486	831.664223	18.760115	-0.045533	1.728218
243.494229	823.786058	18.765120	-0.045521	1.721771
243.525999	815.931854	18.770125	-0.045522	1.715329
243.220093	808.071874	18.775130	-0.045460	1.708814
243.052988	800.196331	18.780135	-0.045424	1.702278
243.218141	792.302688	18.785139	-0.045449	1.695747
242.895503	784.447647	18.790144	-0.045384	1.689157
242.921309	776.568441	18.795149	-0.045383	1.682568
242.859463	768.709220	18.800154	-0.045367	1.675958
242.729462	760.831768	18.805159	-0.045337	1.669298
242.743235	752.962283	18.810163	-0.045335	1.662636
242.702698	745.100449	18.815168	-0.045322	1.655948
242.588855	737.239494	18.820173	-0.045296	1.649222
242.498364	729.383491	18.825178	-0.045274	1.642477
242.454015	721.525462	18.830183	-0.045260	1.635708
242.403450	713.617113	18.835187	-0.045246	1.628867
242.284842	705.762898	18.840192	-0.045218	1.622035
242.311544	697.912150	18.845197	-0.045218	1.615196
242.227222	690.060187	18.850202	-0.045197	1.608313
242.209514	682.210444	18.855207	-0.045189	1.601410
242.100198	674.395788	18.860211	-0.045163	1.594496
241.937890	666.534523	18.865216	-0.045128	1.587503
241.890818	658.698547	18.870221	-0.045114	1.580518
241.741663	650.881597	18.875226	-0.045081	1.573505
241.512792	643.048137	18.880231	-0.045033	1.566433
241.658213	635.193222	18.885235	-0.045055	1.559364
241.649061	627.331687	18.890240	-0.045048	1.552235
241.505230	619.505775	18.895245	-0.045017	1.545085
241.628575	611.648182	18.900250	-0.045034	1.537913
241.490206	603.825959	18.905255	-0.045003	1.530700
241.420836	596.013449	18.910259	-0.044985	1.523473
241.311135	588.203961	18.915264	-0.044960	1.516208
241.191889	580.389916	18.920269	-0.044932	1.508902
241.080558	572.574754	18.925274	-0.044907	1.501561
241.072627	564.753524	18.930279	-0.044900	1.494194
240.925009	556.946721	18.935283	-0.044867	1.486782
240.740883	549.158542	18.940288	-0.044828	1.479346
240.679969	541.325295	18.945293	-0.044811	1.471847
240.662872	533.480678	18.950298	-0.044803	1.464307
240.494326	525.702380	18.955303	-0.044767	1.456767
240.397502	517.904235	18.960307	-0.044743	1.449180
240.262556	510.114450	18.965312	-0.044713	1.441555
240.109720	502.346196	18.970317	-0.044680	1.433908
239.934921	494.558064	18.975322	-0.044642	1.426197
240.047983	486.749243	18.980327	-0.044658	1.418470
240.127688	478.934837	18.985331	-0.044668	1.410690
239.838761	471.186456	18.990336	-0.044609	1.402872
239.794456	463.413047	18.995341	-0.044595	1.395026
239.562717	455.643181	19.000346	-0.044547	1.387107
239.409522	447.880248	19.005351	-0.044513	1.379163
239.593736	440.064593	19.010355	-0.044543	1.371177
239.543999	432.293971	19.015360	-0.044528	1.363150
239.515062	424.546241	19.020365	-0.044518	1.355102
239.575809	416.751370	19.025370	-0.044524	1.346974
239.188820	409.070778	19.030375	-0.044447	1.338837
239.200142	401.310373	19.035379	-0.044444	1.330636
238.895157	393.606258	19.040384	-0.044382	1.322388
238.881937	385.844082	19.045389	-0.044374	1.314079
238.771813	377.991169	19.050394	-0.044349	1.305601
238.661798	370.279087	19.055399	-0.044323	1.297220
238.591649	362.561863	19.060403	-0.044305	1.288787
238.476608	354.848528	19.065408	-0.044279	1.280294
238.447095	347.137975	19.070413	-0.044268	1.271764
238.039270	339.497290	19.075418	-0.044187	1.263182
237.811215	331.812319	19.080423	-0.044139	1.254526
237.688382	324.117406	19.085427	-0.044112	1.245819
237.923982	316.366129	19.090432	-0.044150	1.237055
237.929016	308.643057	19.095437	-0.044146	1.228216
237.852259	300.957539	19.100442	-0.044127	1.219341
237.926335	293.254195	19.105447	-0.044136	1.210410
237.832137	285.604016	19.110451	-0.044113	1.201441
237.648135	277.967608	19.115456	-0.044074	1.192402
237.738758	270.282351	19.120461	-0.044086	1.183293
237.459243	262.681752	19.125466	-0.044028	1.174138
237.359597	255.031199	19.130471	-0.044005	1.164888
237.731540	247.345238	19.135475	-0.044069	1.155619
237.345219	239.720719	19.140480	-0.043992	1.146191
237.235606	232.126026	19.145485	-0.043967	1.136781
237.041334	224.527100	19.150490	-0.043926	1.127268
236.932633	216.933734	19.155495	-0.043900	1.117700
236.846782	209.338848	19.160499	-0.043879	1.108053
236.590377	201.767140	19.165504	-0.043827	1.098313
236.651769	194.169914	19.170509	-0.043833	1.088523
236.466136	186.625140	19.175514	-0.043794	1.078657
236.266946	179.069177	19.180519	-0.043751	1.068683
236.341535	171.496499	19.185523	-0.043760	1.058655
236.146217	163.971932	19.190528	-0.043719	1.048533
236.038234	156.450079	19.195533	-0.043694	1.038336
236.004618	148.931457	19.200538	-0.043683	1.028061
235.941786	141.421600	19.205543	-0.043666	1.017687
235.864479	133.930670	19.210547	-0.043647	1.007229
235.513712	126.499903	19.215552	-0.043577	0.996679
235.362458	119.005751	19.220557	-0.043544	0.985974
235.385990	111.529120	19.225562	-0.043543	0.975222
235.095457	104.112453	19.230567	-0.043484	0.964358
235.113977	96.682967	19.235571	-0.043483	0.953430
234.869352	89.286218	19.240576	-0.043432	0.942356
234.702294	81.913817	19.245581	-0.043396	0.931207
234.442986	74.557694	19.250586	-0.043343	0.919924
234.275927	67.200442	19.255591	-0.043307	0.908523
234.197077	60.086647	19.260595	-0.043288	0.897385