Tue Mar 23 10:30:09 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.677289	0.008870	0.000000	0.000014	0.719905

0.656336	0.067892	0.005005	0.000017	0.720014
0.728043	-0.004061	0.010010	0.000004	0.719897
0.658511	0.012886	0.015014	0.000017	0.719906
0.572332	0.023770	0.020019	0.000033	0.719897
0.788509	-0.011461	0.025024	-0.000007	0.719903
0.509236	0.037486	0.030029	0.000045	0.719901
0.565088	0.023279	0.035034	0.000035	0.719893
0.881473	-0.026865	0.040038	-0.000024	0.719905
0.570189	0.024931	0.045043	0.000034	0.719898
0.737118	-0.001452	0.050048	0.000003	0.719904
0.587833	0.022648	0.055053	0.000031	0.719899
0.680074	0.005722	0.060058	0.000014	0.719898
0.574964	0.028569	0.065062	0.000033	0.719906
0.477942	0.042215	0.070067	0.000051	0.719899
0.513583	0.038931	0.075072	0.000045	0.719905
0.578637	-0.013063	0.080077	0.000033	0.719825
0.542875	-0.122148	0.085082	0.000040	0.719597
0.587696	-0.125129	0.090086	0.000031	0.719607
0.364021	-0.088692	0.095091	0.000073	0.719600
0.515417	-0.112866	0.100096	0.000045	0.719606
0.485115	-0.109475	0.105101	0.000051	0.719602
0.761978	-0.158878	0.110106	-0.000001	0.719601
0.744204	-0.255859	0.115110	0.000003	0.719404
0.652956	-0.308873	0.120115	0.000020	0.719267
0.819103	-0.334369	0.125120	-0.000011	0.719275
0.829464	-0.336280	0.130125	-0.000013	0.719275
0.292426	-0.243528	0.135130	0.000087	0.719269
0.379387	-0.364015	0.140134	0.000071	0.719062
0.296430	-0.400085	0.145139	0.000086	0.718961
0.354155	-0.407701	0.150144	0.000076	0.718966
0.490162	-0.431866	0.155149	0.000050	0.718966
0.438117	-0.469717	0.160154	0.000060	0.718873
0.486891	-0.592438	0.165158	0.000051	0.718648
0.204798	-0.546895	0.170163	0.000104	0.718639
0.260158	-0.552669	0.175168	0.000094	0.718647
0.342948	-0.614667	0.180173	0.000078	0.718553
0.375631	-0.722618	0.185178	0.000072	0.718351
0.471042	-0.736158	0.190182	0.000055	0.718358
0.520928	-0.748900	0.195187	0.000045	0.718350
0.545817	-0.904370	0.200192	0.000041	0.718052
0.521363	-0.915680	0.205197	0.000045	0.718021
0.494241	-0.914746	0.210202	0.000051	0.718013
0.472784	-1.038483	0.215206	0.000055	0.717761
0.193677	-1.020977	0.220211	0.000107	0.717697
0.312562	-1.039016	0.225216	0.000085	0.717703
0.338473	-1.182734	0.230221	0.000080	0.717428
0.189853	-1.181782	0.235226	0.000108	0.717377
0.092236	-1.161030	0.240230	0.000126	0.717384
0.050792	-1.306651	0.245235	0.000134	0.717081
0.071919	-1.308192	0.250240	0.000130	0.717085
0.095464	-1.356817	0.255245	0.000126	0.716997
0.106053	-1.482885	0.260250	0.000124	0.716751
0.106253	-1.479636	0.265254	0.000124	0.716758
-0.029273	-1.569158	0.270259	0.000149	0.716532
0.000937	-1.616886	0.275264	0.000144	0.716448
0.213830	-1.694466	0.280269	0.000104	0.716370
0.050245	-1.786610	0.285274	0.000135	0.716129
0.080147	-1.786920	0.290278	0.000129	0.716139
0.157814	-1.921400	0.295283	0.000115	0.715900
0.051424	-1.908856	0.300288	0.000135	0.715887
-0.071534	-2.003783	0.305293	0.000158	0.715655
0.040542	-2.080603	0.310298	0.000137	0.715543
0.002989	-2.153584	0.315302	0.000144	0.715384
-0.342119	-2.171493	0.320307	0.000208	0.715227
-0.400350	-2.214326	0.325312	0.000219	0.715121
-0.875416	-2.237209	0.330317	0.000308	0.714908
-1.955071	-2.048036	0.335322	0.000509	0.714901
-1.864029	-2.199700	0.340326	0.000492	0.714632
-2.795059	-2.049218	0.345331	0.000665	0.714602
-2.948739	-2.037039	0.350336	0.000694	0.714572
-3.054366	-2.166648	0.355341	0.000714	0.714277
-3.406311	-2.107244	0.360346	0.000779	0.714270
-3.593651	-2.072053	0.365350	0.000814	0.714273
-4.012759	-2.152668	0.370355	0.000892	0.713965
-4.284859	-2.100416	0.375360	0.000943	0.713972
-4.739256	-2.020169	0.380365	0.001028	0.713971
-4.530682	-2.147406	0.385370	0.000989	0.713791
-5.164860	-2.101189	0.390374	0.001107	0.713659
-5.613909	-2.024952	0.395379	0.001191	0.713651
-5.578547	-2.029001	0.400384	0.001184	0.713655
-5.453070	-2.134215	0.405389	0.001161	0.713491
-6.593249	-1.997240	0.410394	0.001373	0.713359
-6.379891	-2.029898	0.415398	0.001334	0.713369
-6.157695	-2.075507	0.420403	0.001292	0.713357
-6.377125	-2.060058	0.425408	0.001333	0.713310
-7.251609	-2.046310	0.430413	0.001496	0.713027
-7.466542	-2.011183	0.435418	0.001536	0.713021
-7.336633	-2.029724	0.440422	0.001512	0.713030
-7.089231	-2.078135	0.445427	0.001466	0.713021
-7.218824	-2.081147	0.450432	0.001490	0.712969
-7.842220	-2.099082	0.455437	0.001606	0.712712
-8.005898	-2.072105	0.460442	0.001637	0.712708
-8.277328	-2.018290	0.465446	0.001687	0.712719
-8.305853	-2.020014	0.470451	0.001693	0.712705
-7.981811	-2.073886	0.475456	0.001633	0.712713
-8.612369	-2.104949	0.480461	0.001750	0.712427
-9.191377	-2.021255	0.485466	0.001858	0.712388
-8.779241	-2.091686	0.490470	0.001781	0.712394
-9.142720	-2.030209	0.495475	0.001849	0.712387
-9.370168	-1.987404	0.500480	0.001891	0.712392
-9.065281	-2.045740	0.505485	0.001835	0.712383
-9.842328	-2.054863	0.510490	0.001979	0.712089
-9.812376	-2.056230	0.515494	0.001974	0.712097
-10.088133	-2.011749	0.520499	0.002025	0.712088
-9.652671	-2.087748	0.525504	0.001944	0.712091
-9.825122	-2.055093	0.530509	0.001976	0.712095
-10.199632	-1.991061	0.535514	0.002046	0.712089
-10.201430	-2.137330	0.540518	0.002047	0.711797
-10.932495	-2.025076	0.545523	0.002183	0.711761
-10.936990	-2.022813	0.550528	0.002184	0.711764
-10.425525	-2.111611	0.555533	0.002088	0.711768
-10.720408	-2.063758	0.560538	0.002143	0.711759
-10.785396	-2.048136	0.565542	0.002156	0.711767
-11.147007	-2.102847	0.570547	0.002223	0.711529
-11.878295	-2.008421	0.575552	0.002359	0.711457
-11.626089	-2.053810	0.580557	0.002312	0.711456
-11.759285	-2.033586	0.585562	0.002337	0.711449
-11.859309	-2.009571	0.590566	0.002356	0.711461
-11.963451	-1.995854	0.595571	0.002375	0.711452
-11.886273	-2.007439	0.600576	0.002361	0.711456
-11.938022	-2.131886	0.605581	0.002371	0.711189
-12.428337	-2.071496	0.610586	0.002462	0.711135
-12.616236	-2.033821	0.615590	0.002497	0.711143
-12.497973	-2.059374	0.620595	0.002475	0.711134
-12.531396	-2.051060	0.625600	0.002481	0.711139
-12.498742	-2.055495	0.630605	0.002475	0.711141
-12.815408	-2.047231	0.635610	0.002534	0.711045
-13.474345	-2.013781	0.640614	0.002657	0.710877
-13.312162	-2.046337	0.645619	0.002627	0.710870
-13.515293	-2.006731	0.650624	0.002665	0.710877
-13.244910	-2.055438	0.655629	0.002614	0.710876
-13.317320	-2.047057	0.660634	0.002628	0.710866
-13.443949	-2.019323	0.665638	0.002652	0.710877
-13.568602	-2.114647	0.670643	0.002675	0.710642
-14.458850	-2.010321	0.675648	0.002841	0.710533
-14.251081	-2.045959	0.680653	0.002802	0.710536
-14.487800	-2.007831	0.685658	0.002846	0.710528
-14.260422	-2.043251	0.690662	0.002804	0.710538
-14.018506	-2.089543	0.695667	0.002759	0.710531
-14.525423	-1.997414	0.700672	0.002853	0.710535
-14.695530	-2.098559	0.705677	0.002885	0.710272
-15.379698	-2.005461	0.710682	0.003013	0.710214
-15.362262	-2.004220	0.715686	0.003009	0.710223
-15.489078	-1.984695	0.720691	0.003033	0.710217
-15.368741	-2.004209	0.725696	0.003011	0.710220
-15.224931	-2.027905	0.730701	0.002984	0.710224
-15.585118	-1.966643	0.735706	0.003051	0.710218
-15.310410	-2.086439	0.740710	0.003000	0.710077
-16.521590	-1.961761	0.745715	0.003226	0.709894
-16.540976	-1.956498	0.750720	0.003229	0.709898
-16.200803	-2.017877	0.755725	0.003166	0.709896
-16.189051	-2.022415	0.760730	0.003164	0.709891
-16.167800	-2.020100	0.765734	0.003160	0.709903
-16.422998	-1.978986	0.770739	0.003207	0.709894
-16.212790	-2.015451	0.775744	0.003168	0.709896
-16.583381	-2.097329	0.780749	0.003238	0.709600
-17.258112	-1.980873	0.785754	0.003363	0.709593
-16.984158	-2.023588	0.790758	0.003312	0.709605
-16.750564	-2.071477	0.795763	0.003269	0.709592
-17.134842	-2.000338	0.800768	0.003340	0.709597
-17.215713	-1.984744	0.805773	0.003355	0.709600
-16.918971	-2.068149	0.810778	0.003300	0.709538
-17.606321	-2.079352	0.815782	0.003428	0.709271
-17.951604	-2.021907	0.820787	0.003493	0.709262
-18.361766	-1.947092	0.825792	0.003569	0.709266
-18.025443	-2.004940	0.830797	0.003507	0.709270
-18.281758	-1.963815	0.835802	0.003554	0.709261
-17.965730	-2.014772	0.840806	0.003496	0.709271
-17.904171	-2.029899	0.845811	0.003484	0.709263
-18.865660	-1.999133	0.850816	0.003663	0.708981
-19.224364	-1.947166	0.855821	0.003730	0.708957
-19.046298	-1.981766	0.860826	0.003697	0.708951
-18.660472	-2.045436	0.865830	0.003625	0.708962
-19.170255	-1.958909	0.870835	0.003720	0.708953
-19.261872	-1.941011	0.875840	0.003737	0.708956
-18.573468	-2.061872	0.880845	0.003609	0.708959
-19.103544	-2.033575	0.885850	0.003708	0.708827
-20.193896	-1.930864	0.890854	0.003911	0.708643
-19.441174	-2.067981	0.895859	0.003771	0.708637
-19.745421	-2.013323	0.900864	0.003828	0.708638
-20.090387	-1.949072	0.905869	0.003892	0.708643
-19.752340	-2.013036	0.910874	0.003829	0.708636
-19.778103	-2.005626	0.915878	0.003834	0.708641
-19.865006	-2.029353	0.920883	0.003850	0.708563
-20.757464	-1.976391	0.925888	0.004016	0.708350
-20.244985	-2.068440	0.930893	0.003921	0.708348
-20.807514	-1.969975	0.935898	0.004026	0.708345
-20.601629	-2.001783	0.940902	0.003987	0.708354
-20.239305	-2.068671	0.945907	0.003920	0.708350
-20.508584	-2.019620	0.950912	0.003970	0.708352
-20.640339	-2.102143	0.955917	0.003995	0.708139
-21.730007	-1.973688	0.960922	0.004198	0.708007
-21.172836	-2.068021	0.965926	0.004094	0.708017
-21.551817	-2.001911	0.970931	0.004165	0.708014
-21.719000	-1.972689	0.975936	0.004196	0.708013
-21.285702	-2.047983	0.980941	0.004115	0.708016
-21.429839	-2.025552	0.985946	0.004142	0.708010
-22.058232	-2.030761	0.990950	0.004259	0.707775
-22.471628	-1.995514	0.995955	0.004336	0.707698
-22.185476	-2.045521	1.000960	0.004283	0.707699
-22.238733	-2.032010	1.005965	0.004293	0.707707
-22.552666	-1.979279	1.010970	0.004351	0.707701
-22.167723	-2.045414	1.015974	0.004280	0.707706
-22.434489	-2.002256	1.020979	0.004330	0.707697
-23.002116	-2.021892	1.025984	0.004435	0.707454
-23.250872	-2.012778	1.030989	0.004482	0.707383
-23.360374	-1.997098	1.035994	0.004502	0.707376
-23.510468	-1.967420	1.040998	0.004530	0.707381
-23.670121	-1.940315	1.046003	0.004560	0.707379
-23.484747	-1.972792	1.051008	0.004525	0.707380
-23.343589	-1.995873	1.056013	0.004499	0.707384
-23.531472	-1.990993	1.061018	0.004534	0.707326
-23.834776	-2.055722	1.066022	0.004591	0.707088
-24.073029	-2.017135	1.071027	0.004635	0.707080
-24.744662	-1.895910	1.076032	0.004760	0.707083
-23.878463	-2.047778	1.081037	0.004599	0.707088
-23.832051	-2.061593	1.086042	0.004591	0.707076
-24.158829	-1.997201	1.091046	0.004651	0.707089
-24.119112	-2.070487	1.096051	0.004644	0.706955
-25.149276	-1.987742	1.101056	0.004836	0.706753
-24.972548	-2.018020	1.106061	0.004803	0.706755
-25.123689	-1.994838	1.111066	0.004831	0.706747
-24.990045	-2.012931	1.116070	0.004806	0.706759
-24.933474	-2.027000	1.121075	0.004796	0.706751
-25.229824	-1.974288	1.126080	0.004851	0.706750
-24.976001	-2.079601	1.131085	0.004804	0.706630
-25.930677	-2.004199	1.136090	0.004982	0.706439
-25.864625	-2.009977	1.141094	0.004970	0.706451
-26.245855	-1.945242	1.146099	0.005041	0.706444
-25.983494	-1.992647	1.151104	0.004992	0.706443
-25.995208	-1.987982	1.156109	0.004994	0.706448
-26.281233	-1.940215	1.161114	0.005047	0.706442
-25.952573	-2.020402	1.166118	0.004986	0.706398
-26.520283	-2.054608	1.171123	0.005092	0.706126
-26.856318	-1.994393	1.176128	0.005155	0.706126
-26.671497	-2.025107	1.181133	0.005120	0.706131
-26.585508	-2.043911	1.186138	0.005104	0.706124
-26.653806	-2.027533	1.191142	0.005117	0.706132
-27.000352	-1.968705	1.196147	0.005182	0.706126
-26.872801	-2.044086	1.201152	0.005158	0.706020
-27.681449	-1.974910	1.206157	0.005309	0.705869
-27.685600	-1.979277	1.211162	0.005309	0.705859
-27.315857	-2.042058	1.216166	0.005241	0.705865
-27.575164	-1.998349	1.221171	0.005289	0.705860
-27.986724	-1.925565	1.226176	0.005366	0.705858
-27.680904	-1.974548	1.231181	0.005309	0.705869
-27.575356	-2.075273	1.236186	0.005289	0.705704
-28.761824	-1.953415	1.241190	0.005510	0.705524
-28.533820	-1.995939	1.246195	0.005468	0.705520
-28.475334	-2.004837	1.251200	0.005457	0.705523
-28.525460	-1.994221	1.256205	0.005466	0.705526
-28.641769	-1.978168	1.261210	0.005488	0.705517
-28.437427	-2.006897	1.266214	0.005450	0.705532
-28.619538	-2.052938	1.271219	0.005484	0.705374
-29.884000	-1.908293	1.276224	0.005719	0.705211
-29.395088	-1.992553	1.281229	0.005629	0.705217
-29.682404	-1.945243	1.286234	0.005682	0.705209
-29.935112	-1.895226	1.291238	0.005729	0.705219
-29.685696	-1.943775	1.296243	0.005683	0.705211
-29.389786	-1.997085	1.301248	0.005628	0.705210
-29.289688	-2.020183	1.306253	0.005609	0.705199
-30.610933	-1.940632	1.311258	0.005855	0.704885
-30.414508	-1.972568	1.316262	0.005819	0.704891
-30.423911	-1.971575	1.321267	0.005821	0.704889
-30.571440	-1.948364	1.326272	0.005848	0.704883
-30.346722	-1.984569	1.331277	0.005806	0.704891
-30.412659	-1.976715	1.336282	0.005819	0.704883
-30.170582	-2.015549	1.341286	0.005774	0.704891
-30.550841	-2.059928	1.346291	0.005844	0.704665
-31.607850	-1.909069	1.351296	0.006041	0.704589
-31.177187	-1.982915	1.356301	0.005961	0.704595
-31.268845	-1.970822	1.361306	0.005978	0.704586
-31.392647	-1.941500	1.366310	0.006001	0.704601
-31.310462	-1.957877	1.371315	0.005986	0.704597
-31.599611	-1.909189	1.376320	0.006040	0.704591
-31.560543	-2.004878	1.381325	0.006033	0.704412
-32.525528	-1.909884	1.386330	0.006213	0.704257
-32.045294	-1.990285	1.391334	0.006123	0.704267
-32.301719	-1.948821	1.396339	0.006171	0.704259
-32.477570	-1.915797	1.401344	0.006204	0.704262
-31.870102	-2.022941	1.406349	0.006091	0.704264
-32.404471	-1.932049	1.411354	0.006190	0.704255
-32.168979	-2.019639	1.416358	0.006147	0.704163
-32.880132	-1.997637	1.421363	0.006279	0.703952
-32.952915	-1.985462	1.426368	0.006293	0.703950
-32.999762	-1.975008	1.431373	0.006301	0.703954
-32.905198	-1.996182	1.436378	0.006284	0.703945
-32.488011	-2.066007	1.441382	0.006206	0.703954
-32.975289	-1.980488	1.446387	0.006297	0.703952
-33.528439	-2.015117	1.451392	0.006400	0.703683
-33.624061	-2.018513	1.456397	0.006418	0.703641
-34.041241	-1.949237	1.461402	0.006496	0.703631
-33.804535	-1.987280	1.466406	0.006452	0.703639
-33.749259	-1.998782	1.471411	0.006441	0.703636
-33.848843	-1.982872	1.476416	0.006460	0.703632
-33.985012	-1.954177	1.481421	0.006485	0.703641
-34.474418	-2.007216	1.486426	0.006577	0.703357
-34.719991	-1.970267	1.491430	0.006622	0.703344
-35.214190	-1.883316	1.496435	0.006714	0.703341
-34.720295	-1.970803	1.501440	0.006623	0.703342
-34.409222	-2.025352	1.506445	0.006565	0.703344
-34.952917	-1.928997	1.511450	0.006666	0.703343
-34.901484	-1.935562	1.516454	0.006656	0.703348
-34.811250	-2.077147	1.521459	0.006640	0.703094
-35.889001	-1.930286	1.526464	0.006840	0.703003
-35.870003	-1.929912	1.531469	0.006837	0.703010
-35.819636	-1.943318	1.536474	0.006828	0.703001
-35.474389	-2.001180	1.541478	0.006763	0.703008
-35.584008	-1.981276	1.546483	0.006784	0.703009
-35.864632	-1.933709	1.551488	0.006836	0.703004
-35.874296	-2.034019	1.556493	0.006838	0.702798
-36.915934	-1.901565	1.561498	0.007032	0.702690
-36.809998	-1.915841	1.566502	0.007012	0.702699
-36.609680	-1.953197	1.571507	0.006975	0.702696
-36.720160	-1.935225	1.576512	0.006996	0.702692
-36.512207	-1.968383	1.581517	0.006957	0.702700
-36.800490	-1.923811	1.586522	0.007011	0.702686
-36.431609	-2.038746	1.591526	0.006942	0.702587
-37.415903	-1.967945	1.596531	0.007125	0.702375
-37.574104	-1.941194	1.601536	0.007155	0.702372
-37.123568	-2.019183	1.606541	0.007071	0.702376
-37.373797	-1.980387	1.611546	0.007118	0.702364
-37.335417	-1.983085	1.616550	0.007111	0.702373
-37.199908	-2.008077	1.621555	0.007086	0.702371
-37.511941	-2.047365	1.626560	0.007144	0.702179
-38.159901	-1.981295	1.631565	0.007264	0.702079
-38.238904	-1.970746	1.636570	0.007279	0.702071
-38.271717	-1.958902	1.641574	0.007285	0.702084
-38.296180	-1.956918	1.646579	0.007290	0.702079
-38.585849	-1.908426	1.651584	0.007344	0.702072
-38.008843	-2.006186	1.656589	0.007237	0.702082
-38.617340	-2.036889	1.661594	0.007350	0.701801
-39.506608	-1.902936	1.666598	0.007515	0.701751
-39.257769	-1.948211	1.671603	0.007469	0.701749
-38.844136	-2.023597	1.676608	0.007392	0.701745
-39.045206	-1.983070	1.681613	0.007430	0.701755
-39.335629	-1.938027	1.686618	0.007484	0.701741
-38.933289	-2.004537	1.691622	0.007409	0.701751
-39.490991	-2.040640	1.696627	0.007513	0.701477
-40.363499	-1.903686	1.701632	0.007675	0.701439
-39.996439	-1.967147	1.706637	0.007607	0.701443
-39.922107	-1.985434	1.711642	0.007593	0.701433
-39.970494	-1.971859	1.716646	0.007602	0.701443
-39.825068	-1.999006	1.721651	0.007575	0.701440
-39.877500	-1.991994	1.726656	0.007585	0.701435
-40.417806	-2.046234	1.731661	0.007686	0.701130
-40.785463	-1.986719	1.736666	0.007754	0.701118
-40.793010	-1.981545	1.741670	0.007756	0.701125
-40.615895	-2.014996	1.746675	0.007723	0.701122
-40.833051	-1.977382	1.751680	0.007763	0.701119
-40.774305	-1.984836	1.756685	0.007753	0.701125
-40.794756	-2.028325	1.761690	0.007756	0.701030
-41.777895	-1.928048	1.766694	0.007940	0.700877
-41.475553	-1.983711	1.771699	0.007883	0.700874
-41.330223	-2.011340	1.776704	0.007856	0.700870
-41.249162	-2.020965	1.781709	0.007841	0.700880
-41.609642	-1.961069	1.786714	0.007908	0.700871
-41.730775	-1.936377	1.791718	0.007931	0.700877
-41.805921	-2.062298	1.796723	0.007945	0.700595
-42.558993	-1.958383	1.801728	0.008085	0.700533
-42.476594	-1.968596	1.806733	0.008070	0.700542
-42.068467	-2.047314	1.811738	0.007994	0.700530
-42.339115	-1.994233	1.816742	0.008045	0.700539
-42.295329	-2.003565	1.821747	0.008037	0.700536
-42.445981	-2.036882	1.826752	0.008065	0.700414
-43.373388	-1.965317	1.831757	0.008237	0.700224
-43.577483	-1.931798	1.836762	0.008275	0.700218
-43.391019	-1.962106	1.841766	0.008241	0.700224
-43.118725	-2.012411	1.846771	0.008190	0.700220
-43.377841	-1.968389	1.851776	0.008238	0.700215
-43.576676	-1.927537	1.856781	0.008275	0.700226
-43.443627	-1.986906	1.861786	0.008251	0.700154
-44.183144	-1.977720	1.866790	0.008389	0.699905
-44.206748	-1.975227	1.871795	0.008393	0.699901
-44.441129	-1.935883	1.876800	0.008437	0.699896
-43.903407	-2.027440	1.881805	0.008337	0.699905
-44.278117	-1.966150	1.886810	0.008406	0.699893
-44.160642	-1.982967	1.891814	0.008385	0.699902
-44.253207	-2.016048	1.896819	0.008402	0.699801
-45.431475	-1.905464	1.901824	0.008621	0.699599
-45.030502	-1.974178	1.906829	0.008547	0.699604
-44.962753	-1.992240	1.911834	0.008534	0.699592
-45.104094	-1.963257	1.916838	0.008561	0.699600
-44.880511	-2.003608	1.921843	0.008519	0.699599
-45.038973	-1.976223	1.926848	0.008549	0.699597
-44.950259	-2.063354	1.931853	0.008532	0.699452
-46.384892	-1.900163	1.936858	0.008799	0.699263
-45.773513	-2.006744	1.941862	0.008686	0.699268
-45.696771	-2.021144	1.946867	0.008671	0.699267
-45.961617	-1.975325	1.951872	0.008721	0.699264
-45.732718	-2.011439	1.956877	0.008678	0.699273
-45.827774	-1.998855	1.961882	0.008696	0.699264
-46.131029	-2.049779	1.966886	0.008752	0.699051
-46.968815	-1.945265	1.971891	0.008908	0.698959
-46.845884	-1.971318	1.976896	0.008886	0.698951
-46.534605	-2.022086	1.981901	0.008828	0.698960
-47.187955	-1.910253	1.986906	0.008949	0.698951
-46.960846	-1.947703	1.991910	0.008907	0.698957
-46.522415	-2.025944	1.996915	0.008826	0.698957
-47.419494	-1.992378	2.001920	0.008993	0.698700

-47.545021	-2.000556	2.011917	0.009016	0.698637
-47.797326	-1.956343	2.021914	0.009063	0.698636
-47.557900	-1.998701	2.031910	0.009019	0.698636
-47.844994	-1.945441	2.041907	0.009072	0.698640
-47.640310	-1.980989	2.051904	0.009034	0.698642
-47.815390	-1.951315	2.061901	0.009067	0.698638
-47.765137	-1.959709	2.071898	0.009058	0.698639
-47.561492	-1.994226	2.081894	0.009020	0.698643
-47.515437	-2.002371	2.091891	0.009012	0.698643
-47.687538	-1.971269	2.101888	0.009044	0.698643
-47.562367	-1.994329	2.111885	0.009020	0.698642
-47.583703	-1.930579	2.121882	0.009025	0.698763
-46.658557	-1.999184	2.131878	0.008852	0.698959
-46.874460	-1.960195	2.141875	0.008893	0.698960
-46.945279	-1.946385	2.151872	0.008906	0.698962
-46.810470	-1.970509	2.161869	0.008881	0.698961
-47.157267	-1.872499	2.171866	0.008946	0.699035
-45.982338	-1.964408	2.181862	0.008727	0.699274
-46.107904	-1.942720	2.191859	0.008750	0.699272
-45.883472	-1.984326	2.201856	0.008709	0.699268
-46.009948	-1.961206	2.211853	0.008732	0.699269
-45.195651	-1.949053	2.221850	0.008581	0.699589
-44.911877	-1.992349	2.231846	0.008528	0.699603
-44.896975	-1.995670	2.241843	0.008526	0.699602
-44.966705	-1.983824	2.251840	0.008539	0.699600
-44.340046	-1.990222	2.261837	0.008422	0.699814
-44.227683	-1.970074	2.271834	0.008401	0.699895
-44.158145	-1.981481	2.281830	0.008388	0.699897
-44.110067	-1.990179	2.291827	0.008380	0.699897
-43.381595	-1.990879	2.301824	0.008244	0.700159
-43.344517	-1.967224	2.311821	0.008237	0.700220
-43.245455	-1.986168	2.321818	0.008219	0.700217
-43.328757	-1.952642	2.331814	0.008235	0.700255
-42.483600	-1.966329	2.341811	0.008077	0.700532
-42.255440	-2.005131	2.351808	0.008035	0.700536
-42.543387	-1.953685	2.361805	0.008089	0.700536
-42.130380	-1.948589	2.371802	0.008012	0.700695
-41.206790	-2.024058	2.381798	0.007840	0.700876
-41.471048	-1.976721	2.391795	0.007889	0.700876
-41.429425	-1.984885	2.401792	0.007882	0.700875
-41.069865	-1.948427	2.411789	0.007815	0.701078
-40.816937	-1.971700	2.421786	0.007768	0.701122
-40.599414	-2.010492	2.431782	0.007728	0.701122
-40.559696	-1.946834	2.441779	0.007720	0.701265
-39.598892	-2.032676	2.451776	0.007541	0.701438
-40.067276	-1.948987	2.461773	0.007629	0.701438
-39.782477	-2.000467	2.471770	0.007576	0.701436
-39.035797	-1.981594	2.481766	0.007437	0.701744
-38.949940	-1.995560	2.491763	0.007421	0.701746
-38.839522	-2.015525	2.501760	0.007401	0.701746
-38.785779	-1.940593	2.511757	0.007391	0.701916
-37.970603	-2.008455	2.521754	0.007239	0.702073
-38.154342	-1.974202	2.531750	0.007273	0.702076
-38.140144	-1.965618	2.541747	0.007271	0.702098
-37.294868	-1.981635	2.551744	0.007114	0.702370
-37.170766	-2.005508	2.561741	0.007091	0.702367
-37.311521	-1.980696	2.571738	0.007117	0.702366
-36.970493	-1.934867	2.581734	0.007053	0.702581
-36.419472	-1.977207	2.591731	0.006951	0.702694
-36.518742	-1.960835	2.601728	0.006970	0.702691
-36.453661	-1.918547	2.611725	0.006957	0.702800
-35.367283	-2.011630	2.621722	0.006755	0.703003
-35.474355	-1.992669	2.631718	0.006775	0.703002
-35.347249	-2.013945	2.641715	0.006752	0.703005
-35.003104	-1.942720	2.651712	0.006688	0.703272
-34.803287	-1.945109	2.661709	0.006651	0.703339
-34.776052	-1.950477	2.671706	0.006646	0.703338
-34.597235	-1.914284	2.681702	0.006613	0.703475
-33.728099	-1.990601	2.691699	0.006451	0.703634
-33.925850	-1.955322	2.701696	0.006488	0.703634
-33.963897	-1.932482	2.711693	0.006495	0.703666
-32.940736	-1.974687	2.721690	0.006305	0.703949
-32.945758	-1.971245	2.731686	0.006306	0.703953
-32.692102	-2.016161	2.741683	0.006259	0.703954
-32.516874	-1.966285	2.751680	0.006226	0.704117
-32.225583	-1.948044	2.761677	0.006172	0.704259
-32.081874	-1.974601	2.771674	0.006145	0.704256
-32.076458	-1.959339	2.781670	0.006144	0.704289
-31.352499	-1.939001	2.791667	0.006010	0.704590
-31.195478	-1.967349	2.801664	0.005981	0.704589
-31.307179	-1.946867	2.811661	0.006001	0.704590
-30.587341	-1.971067	2.821658	0.005868	0.704800
-30.462357	-1.949953	2.831654	0.005844	0.704887
-30.162425	-2.002377	2.841651	0.005789	0.704889
-30.318617	-1.958217	2.851648	0.005818	0.704921
-29.580027	-1.947442	2.861645	0.005680	0.705208
-29.308995	-1.996460	2.871642	0.005630	0.705206
-29.454942	-1.968283	2.881638	0.005657	0.705210
-28.872330	-1.978326	2.891635	0.005549	0.705399
-28.677908	-1.949593	2.901632	0.005513	0.705526
-28.592061	-1.965448	2.911629	0.005497	0.705525
-28.707304	-1.918438	2.921626	0.005519	0.705578
-27.490852	-1.993738	2.931622	0.005292	0.705863
-27.238443	-2.037531	2.941619	0.005245	0.705865
-27.583403	-1.977147	2.951616	0.005310	0.705863
-27.428834	-1.966326	2.961613	0.005281	0.705939
-26.697228	-2.004370	2.971610	0.005145	0.706125
-26.907667	-1.965748	2.981606	0.005184	0.706127
-26.675750	-2.006355	2.991603	0.005141	0.706128
-26.300035	-1.936821	3.001600	0.005071	0.706403
-25.845334	-1.996915	3.011597	0.004987	0.706444
-26.076401	-1.955395	3.021594	0.005030	0.706445
-25.574224	-1.969588	3.031590	0.004936	0.706596
-24.954449	-2.002816	3.041587	0.004821	0.706751
-25.267156	-1.946474	3.051584	0.004879	0.706752
-24.874396	-2.009947	3.061581	0.004806	0.706765
-24.536780	-1.914191	3.071578	0.004744	0.707078
-23.953862	-2.015246	3.081574	0.004635	0.707083
-24.054149	-1.998357	3.091571	0.004654	0.707081
-23.781141	-1.967547	3.101568	0.004603	0.707241
-23.397126	-1.968297	3.111565	0.004532	0.707376
-23.422251	-1.963986	3.121562	0.004537	0.707376
-23.122443	-2.004578	3.131558	0.004481	0.707401
-22.530374	-1.960328	3.141555	0.004371	0.707702
-22.330726	-1.995061	3.151552	0.004334	0.707703
-22.460554	-1.973532	3.161549	0.004358	0.707700
-22.264918	-1.918769	3.171546	0.004322	0.707879
-21.358425	-2.011702	3.181542	0.004153	0.708017
-21.633651	-1.963603	3.191539	0.004204	0.708014
-21.484563	-1.969956	3.201536	0.004177	0.708055
-20.639214	-1.972640	3.211533	0.004020	0.708351
-20.749111	-1.953380	3.221530	0.004040	0.708350
-20.583766	-1.982114	3.231526	0.004009	0.708352
-20.392585	-1.925728	3.241523	0.003974	0.708533
-19.575258	-2.017755	3.251520	0.003822	0.708640
-19.901348	-1.961024	3.261517	0.003883	0.708637
-19.818802	-1.951950	3.271514	0.003867	0.708684
-18.854416	-1.987760	3.281510	0.003688	0.708957
-18.875917	-1.979804	3.291507	0.003692	0.708965
-18.830485	-1.989589	3.301504	0.003684	0.708961
-18.460935	-1.967713	3.311501	0.003615	0.709137
-17.959385	-1.992058	3.321498	0.003522	0.709266
-17.861965	-2.009194	3.331494	0.003504	0.709267
-18.015155	-1.980308	3.341491	0.003532	0.709270
-17.302271	-1.951181	3.351488	0.003400	0.709582
-17.116514	-1.975268	3.361485	0.003365	0.709600
-17.157454	-1.968297	3.371482	0.003373	0.709599
-16.783591	-1.967030	3.381478	0.003303	0.709735
-16.025796	-2.020051	3.391475	0.003163	0.709898
-16.158183	-1.996317	3.401472	0.003187	0.709898
-16.222367	-1.984775	3.411469	0.003199	0.709898
-15.576801	-1.969618	3.421466	0.003079	0.710158
-15.263587	-1.996194	3.431462	0.003021	0.710217
-15.207699	-2.003036	3.441459	0.003011	0.710223
-15.077246	-2.002636	3.451456	0.002987	0.710270
-14.230832	-2.018418	3.461453	0.002829	0.710539
-14.152815	-2.032486	3.471450	0.002815	0.710539
-14.360857	-1.995822	3.481446	0.002853	0.710538
-13.994187	-1.998926	3.491443	0.002785	0.710662
-13.060214	-2.057856	3.501440	0.002612	0.710876
-13.429126	-1.992413	3.511437	0.002680	0.710876
-13.199984	-2.034424	3.521434	0.002638	0.710873
-12.970142	-1.997343	3.531430	0.002595	0.711029
-12.567653	-2.010461	3.541427	0.002520	0.711145
-12.484459	-2.025217	3.551424	0.002505	0.711145
-12.511883	-2.003977	3.561421	0.002510	0.711178
-11.623326	-2.022651	3.571418	0.002345	0.711456
-11.680701	-2.010756	3.581414	0.002356	0.711459
-11.929840	-1.964580	3.591411	0.002402	0.711463
-11.120763	-1.997166	3.601408	0.002252	0.711685
-11.172925	-1.946507	3.611405	0.002261	0.711767
-10.656016	-2.041077	3.621402	0.002165	0.711762
-10.859514	-1.943935	3.631398	0.002203	0.711883
-9.939103	-1.999223	3.641395	0.002032	0.712100
-9.763448	-2.031900	3.651392	0.001999	0.712097
-10.002921	-1.990857	3.661389	0.002044	0.712093
-9.135003	-2.020323	3.671386	0.001883	0.712343
-9.183970	-1.987805	3.681382	0.001892	0.712390
-9.073020	-2.004484	3.691379	0.001871	0.712396
-8.919172	-1.977262	3.701376	0.001843	0.712504
-8.162330	-2.006482	3.711373	0.001702	0.712715
-8.071945	-2.023852	3.721370	0.001685	0.712712
-8.128718	-2.013868	3.731366	0.001696	0.712711
-7.685342	-1.979008	3.741363	0.001613	0.712938
-7.284911	-2.004188	3.751360	0.001539	0.713029
-7.335621	-1.994656	3.761357	0.001548	0.713030
-7.134785	-1.993579	3.771354	0.001511	0.713103
-6.548801	-1.967205	3.781350	0.001402	0.713363
-6.118718	-2.044066	3.791347	0.001322	0.713363
-6.448358	-1.985358	3.801344	0.001384	0.713362
-5.769644	-2.006020	3.811341	0.001257	0.713562
-5.767079	-1.956627	3.821338	0.001257	0.713661
-5.728469	-1.964460	3.831334	0.001250	0.713659
-5.265631	-2.001686	3.841331	0.001164	0.713748
-4.619429	-2.002540	3.851328	0.001044	0.713975
-4.590056	-2.006998	3.861325	0.001038	0.713977
-4.540367	-2.017513	3.871322	0.001029	0.713973
-4.065048	-2.011484	3.881318	0.000941	0.714153
-3.533884	-2.040826	3.891315	0.000842	0.714283
-3.851749	-1.984179	3.901312	0.000901	0.714282
-3.606313	-2.028854	3.911309	0.000856	0.714280
-2.970675	-1.978312	3.921306	0.000737	0.714605
-2.898268	-1.989687	3.931302	0.000724	0.714608
-2.713877	-2.022150	3.941299	0.000690	0.714609
-2.715639	-1.944713	3.951296	0.000690	0.714762
-2.193184	-1.961065	3.961293	0.000593	0.714914
-2.022608	-1.993782	3.971290	0.000562	0.714909
-2.037328	-1.964087	3.981286	0.000564	0.714962
-1.862461	-1.859235	3.991283	0.000532	0.715232
-1.573010	-1.909817	4.001280	0.000478	0.715234
-1.705876	-1.836732	4.011277	0.000503	0.715332
-1.513776	-1.761908	4.021274	0.000467	0.715548
-1.328178	-1.796002	4.031270	0.000433	0.715546
-1.177436	-1.684452	4.041267	0.000405	0.715820
-1.098851	-1.665584	4.051264	0.000390	0.715885
-1.231754	-1.574351	4.061261	0.000415	0.716018
-1.119549	-1.534843	4.071258	0.000394	0.716136
-1.171517	-1.439502	4.081254	0.000404	0.716306
-1.032974	-1.390182	4.091251	0.000378	0.716453
-0.977384	-1.279781	4.101248	0.000368	0.716691
-0.825176	-1.259301	4.111245	0.000340	0.716785
-0.639584	-1.139775	4.121242	0.000305	0.717087
-0.630091	-1.075803	4.131238	0.000303	0.717216
-0.750608	-0.969190	4.141235	0.000326	0.717385
-0.518648	-0.853563	4.151232	0.000283	0.717695
-0.636957	-0.740804	4.161229	0.000305	0.717876
-0.512580	-0.658862	4.171226	0.000282	0.718081
-0.296803	-0.559108	4.181222	0.000242	0.718354
-0.422102	-0.407389	4.191219	0.000265	0.718610
-0.454011	-0.278272	4.201216	0.000271	0.718853
-0.333250	-0.170754	4.211213	0.000248	0.719108
-0.367823	-0.024240	4.221210	0.000255	0.719384
-0.196042	0.091568	4.231206	0.000223	0.719673
0.000000	0.241506	4.241203	0.000186	0.720037

-0.097422	0.875695	4.246208	0.000204	0.721252
-0.088803	2.133124	4.251213	0.000202	0.723725
0.439711	3.893280	4.256218	0.000102	0.727351
0.696191	6.254129	4.261222	0.000053	0.732031
1.097199	9.104954	4.266227	-0.000023	0.737674
1.397891	12.439940	4.271232	-0.000081	0.744164
1.860670	16.212875	4.276237	-0.000170	0.751479
2.424487	20.375489	4.281242	-0.000278	0.759486
3.059328	24.912157	4.286246	-0.000399	0.768124
3.599082	29.859835	4.291251	-0.000502	0.777385
4.189839	35.127017	4.296256	-0.000616	0.787129
4.561553	40.763522	4.301261	-0.000689	0.797343
5.038389	46.676718	4.306266	-0.000781	0.807945
7.002484	52.618935	4.311270	-0.001151	0.818916
8.645529	58.928546	4.316275	-0.001461	0.830272
9.230847	65.642289	4.321280	-0.001574	0.841841
9.871964	72.575864	4.326285	-0.001698	0.853634
10.083802	79.786321	4.331290	-0.001742	0.865596
10.784007	87.083416	4.336294	-0.001877	0.877674
11.989617	94.482856	4.341299	-0.002106	0.889892
13.100212	102.053301	4.346304	-0.002318	0.902187
13.842357	109.855912	4.351309	-0.002461	0.914576
15.241271	117.646531	4.356314	-0.002727	0.926956
16.191561	125.647549	4.361318	-0.002909	0.939372
17.055174	133.779682	4.366323	-0.003075	0.951798
17.801902	142.005721	4.371328	-0.003219	0.964171
18.510603	150.331807	4.376333	-0.003357	0.976523
19.622401	158.670158	4.381338	-0.003569	0.988838
20.555634	167.087252	4.386342	-0.003748	1.001069
21.495176	175.562115	4.391347	-0.003929	1.013234
22.574088	184.044587	4.396352	-0.004135	1.025298
23.220546	192.643771	4.401357	-0.004261	1.037278
24.156021	201.210812	4.406362	-0.004441	1.049145
24.801313	209.842010	4.411366	-0.004566	1.060898
25.414342	218.511229	4.416371	-0.004686	1.072564
26.173921	227.136506	4.421376	-0.004833	1.084081
27.059606	235.770003	4.426381	-0.005004	1.095514
27.750460	244.433693	4.431386	-0.005138	1.106824
28.402218	253.103480	4.436390	-0.005265	1.118019
29.332401	261.729580	4.441395	-0.005443	1.129108
30.158269	270.366984	4.446400	-0.005603	1.140080
30.708051	279.073803	4.451405	-0.005711	1.150974
31.705688	287.672781	4.456410	-0.005902	1.161728
32.306580	296.313456	4.461414	-0.006020	1.172351
33.557838	304.851205	4.466419	-0.006258	1.182888
34.345148	313.469034	4.471424	-0.006410	1.193333
34.852342	322.098022	4.476429	-0.006510	1.203643
35.668903	330.687447	4.481434	-0.006668	1.213881
35.962822	339.326356	4.486438	-0.006728	1.223987
36.973425	347.866949	4.491443	-0.006922	1.234037
37.529590	356.422108	4.496448	-0.007031	1.243935
38.324509	364.936466	4.501453	-0.007184	1.253753
38.959781	373.468141	4.506458	-0.007308	1.263484
39.409117	382.021135	4.511462	-0.007397	1.273129
40.150749	390.500826	4.516467	-0.007541	1.282675
40.603761	399.015828	4.521472	-0.007631	1.292135
41.746774	407.410392	4.526477	-0.007849	1.301521
42.167428	415.995721	4.531482	-0.007933	1.310915
42.692388	424.509486	4.536486	-0.008036	1.320184
43.632881	432.873570	4.541491	-0.008217	1.329302
44.217945	441.293336	4.546496	-0.008331	1.338354
44.699270	449.714141	4.551501	-0.008426	1.347328
45.248138	458.132911	4.556506	-0.008534	1.356252
45.573996	466.545264	4.561510	-0.008600	1.365072
46.086382	474.953176	4.566515	-0.008701	1.373862
46.575544	483.326044	4.571520	-0.008797	1.382557
47.115766	491.706756	4.576525	-0.008903	1.391214
47.653034	500.068758	4.581530	-0.009009	1.399797
47.872567	508.444357	4.586534	-0.009055	1.408289
48.752854	516.745172	4.591539	-0.009224	1.416764
49.169786	525.082809	4.596544	-0.009307	1.425149
49.852419	533.397055	4.601549	-0.009440	1.433505
50.280769	541.722855	4.606554	-0.009525	1.441782
50.927943	549.999545	4.611558	-0.009651	1.449999
51.440353	558.321879	4.616563	-0.009751	1.458193
51.861088	566.630448	4.621568	-0.009835	1.466312
52.776268	574.924834	4.626573	-0.010011	1.474451
53.561538	583.168239	4.631578	-0.010162	1.482476
53.934112	591.464130	4.636582	-0.010237	1.490443
54.358557	599.776700	4.641587	-0.010321	1.498391
55.060582	608.006807	4.646592	-0.010457	1.506263
55.424607	616.317296	4.651597	-0.010531	1.514116
55.796015	624.591976	4.656602	-0.010605	1.521897
56.198144	632.856864	4.661606	-0.010685	1.529634
56.616359	641.144283	4.666611	-0.010769	1.537354
57.080043	649.371439	4.671616	-0.010860	1.544988
57.424650	657.663806	4.676621	-0.010930	1.552626
58.043109	665.860239	4.681626	-0.011050	1.560179
58.460185	674.090502	4.686630	-0.011133	1.567697
59.421606	682.266645	4.691635	-0.011317	1.575209
60.026280	690.484142	4.696640	-0.011435	1.582670
60.425184	698.731363	4.701645	-0.011515	1.590093
60.830483	706.988813	4.706650	-0.011596	1.597492
61.477251	715.163589	4.711654	-0.011721	1.604818
62.346509	723.349214	4.716659	-0.011888	1.612151
62.589992	731.602634	4.721664	-0.011939	1.619422
63.035317	739.818745	4.726669	-0.012027	1.626656
63.384395	748.119033	4.731674	-0.012098	1.633918
63.747972	756.302131	4.736678	-0.012171	1.641048
64.319023	764.477888	4.741683	-0.012282	1.648169
64.889681	772.653449	4.746688	-0.012394	1.655259
65.457192	780.817064	4.751693	-0.012505	1.662308
65.970066	789.016198	4.756698	-0.012606	1.669350
66.182281	797.248307	4.761702	-0.012650	1.676350
66.689245	805.420057	4.766707	-0.012750	1.683309
66.965866	813.618090	4.771712	-0.012807	1.690231
67.238697	821.840192	4.776717	-0.012863	1.697144
67.793128	829.993370	4.781722	-0.012971	1.704009
68.200512	838.173783	4.786726	-0.013053	1.710849
68.546895	846.383171	4.791731	-0.013122	1.717678
69.108402	854.496647	4.796736	-0.013232	1.724428
69.531691	862.668590	4.801741	-0.013316	1.731182
69.940611	870.847782	4.806746	-0.013398	1.737914
70.116614	879.025588	4.811750	-0.013436	1.744589
70.575888	887.193384	4.816755	-0.013526	1.751266
70.984676	895.344740	4.821760	-0.013608	1.757898
71.475630	903.482630	4.826765	-0.013704	1.764505
71.912544	911.661706	4.831770	-0.013791	1.771113
72.213839	919.824693	4.836774	-0.013852	1.777666
72.783120	927.962581	4.841779	-0.013964	1.784209
73.014686	936.171039	4.846784	-0.014012	1.790742
73.555601	944.331341	4.851789	-0.014118	1.797250
74.066113	952.451933	4.856794	-0.014218	1.803701
74.385573	960.591915	4.861798	-0.014283	1.810120
75.134480	968.692903	4.866803	-0.014428	1.816537
75.645968	976.808209	4.871808	-0.014528	1.822915
75.911990	984.983346	4.876813	-0.014583	1.829287
76.498944	993.101961	4.881818	-0.014698	1.835631
76.840031	1001.237828	4.886822	-0.014766	1.841938
77.103473	1009.412803	4.891827	-0.014821	1.848244
77.311500	1017.580298	4.896832	-0.014865	1.854516
77.668356	1025.707595	4.901837	-0.014936	1.860753
78.149964	1033.837924	4.906842	-0.015031	1.866987
78.468059	1042.006361	4.911846	-0.015096	1.873209
79.002256	1050.106200	4.916851	-0.015201	1.879384
79.440499	1058.195604	4.921856	-0.015287	1.885520
79.732061	1066.358651	4.926861	-0.015347	1.891674
80.340303	1074.471061	4.931866	-0.015465	1.897806
80.568976	1082.589256	4.936870	-0.015513	1.903880
80.931549	1090.739043	4.941875	-0.015586	1.909972
81.481237	1098.842377	4.946880	-0.015694	1.916032
82.028201	1106.932026	4.951885	-0.015801	1.922062
82.418512	1115.063314	4.956890	-0.015879	1.928087
82.486104	1123.243354	4.961894	-0.015896	1.934092
83.059439	1131.326737	4.966899	-0.016008	1.940064
83.467446	1139.441254	4.971904	-0.016090	1.946022
83.805591	1147.613215	4.976909	-0.016158	1.951996
84.066843	1155.757275	4.981914	-0.016212	1.957923
84.429003	1163.821118	4.986918	-0.016284	1.963785
84.908254	1171.921444	4.991923	-0.016379	1.969668
85.164818	1180.051942	4.996928	-0.016432	1.975532
85.509318	1188.137171	5.001933	-0.016501	1.981355
85.848425	1196.262413	5.006938	-0.016570	1.987189
86.271911	1204.365036	5.011942	-0.016654	1.992998
86.862114	1212.455063	5.016947	-0.016769	1.998799
87.279679	1220.542944	5.021952	-0.016852	2.004564
87.648894	1228.649649	5.026957	-0.016926	2.010320
88.445900	1236.720981	5.031962	-0.017079	2.016079
88.671104	1244.840628	5.036966	-0.017126	2.021796
89.123085	1252.947614	5.041971	-0.017216	2.027511
89.445293	1261.091790	5.046976	-0.017281	2.033223
89.708261	1269.204001	5.051981	-0.017335	2.038891
89.986529	1277.308594	5.056986	-0.017392	2.044539
90.086890	1285.430472	5.061990	-0.017416	2.050165
90.390271	1293.556858	5.066995	-0.017478	2.055799
90.880892	1301.602765	5.072000	-0.017574	2.061382
91.237288	1309.700494	5.077005	-0.017646	2.066971
91.737447	1317.798363	5.082010	-0.017744	2.072560
91.848860	1325.915695	5.087014	-0.017770	2.078108
92.135683	1334.018090	5.092019	-0.017829	2.083648
92.585593	1342.082470	5.097024	-0.017918	2.089164
93.112688	1350.177216	5.102029	-0.018021	2.094694
93.505150	1358.268094	5.107034	-0.018100	2.100193
93.783616	1366.353547	5.112038	-0.018157	2.105662
94.258037	1374.479015	5.117043	-0.018250	2.111164
94.515654	1382.619249	5.122048	-0.018304	2.116639
95.146423	1390.633491	5.127053	-0.018426	2.122053
95.298555	1398.754350	5.132058	-0.018460	2.127477
95.425705	1406.860607	5.137062	-0.018489	2.132876
96.135001	1414.903644	5.142067	-0.018626	2.138275
96.400785	1422.983969	5.147072	-0.018681	2.143642
96.637163	1431.086594	5.152077	-0.018730	2.149008
96.973389	1439.213239	5.157082	-0.018798	2.154385
97.165818	1447.282576	5.162086	-0.018839	2.159698
97.615419	1455.345381	5.167091	-0.018928	2.165018
98.039740	1463.417120	5.172096	-0.019012	2.170328
98.159055	1471.544554	5.177101	-0.019039	2.175633
98.460198	1479.636824	5.182106	-0.019101	2.180918
98.981445	1487.675145	5.187110	-0.019203	2.186177
99.318842	1495.793274	5.192115	-0.019271	2.191457
99.536645	1503.906932	5.197120	-0.019317	2.196711
99.858855	1511.962823	5.202125	-0.019382	2.201924
100.565494	1519.988108	5.207130	-0.019519	2.207140
100.738608	1528.085415	5.212134	-0.019556	2.212342
101.317262	1536.144536	5.217139	-0.019669	2.217543
101.483129	1544.231566	5.222144	-0.019705	2.222713
101.788098	1552.316133	5.227149	-0.019767	2.227882
102.240311	1560.412932	5.232154	-0.019857	2.233060
102.480798	1568.480881	5.237158	-0.019906	2.238188
102.903991	1576.538357	5.242163	-0.019990	2.243314
103.175976	1584.630405	5.247168	-0.020046	2.248437
103.505639	1592.731116	5.252173	-0.020113	2.253559
103.874520	1600.804205	5.257178	-0.020187	2.258655
103.955071	1608.895039	5.262182	-0.020207	2.263726
104.206288	1616.994492	5.267187	-0.020259	2.268805
104.657917	1625.131010	5.272192	-0.020348	2.273913
105.014976	1633.168478	5.277197	-0.020420	2.278940
105.277961	1641.213984	5.282202	-0.020474	2.283953
105.656029	1649.248154	5.287206	-0.020550	2.288958
105.997238	1657.338141	5.292211	-0.020619	2.293982
106.398466	1665.390969	5.297216	-0.020698	2.298978
106.610265	1673.459333	5.302221	-0.020743	2.303957
107.069715	1681.520616	5.307226	-0.020834	2.308941
107.371777	1689.597397	5.312230	-0.020895	2.313911
107.662095	1697.664969	5.317235	-0.020955	2.318864
107.914827	1705.732046	5.322240	-0.021007	2.323802
108.179028	1713.819276	5.327245	-0.021061	2.328743
108.523666	1721.904461	5.332250	-0.021131	2.333679
108.904085	1729.946176	5.337254	-0.021207	2.338581
109.237828	1738.020918	5.342259	-0.021274	2.343489
109.519184	1746.107989	5.347264	-0.021332	2.348389
109.689754	1754.204000	5.352269	-0.021369	2.353276
110.162670	1762.256190	5.357274	-0.021462	2.358151
110.309065	1770.311435	5.362278	-0.021494	2.362991
110.695965	1778.359610	5.367283	-0.021572	2.367836
111.043744	1786.432407	5.372288	-0.021641	2.372683
111.433280	1794.483573	5.377293	-0.021719	2.377510
111.548807	1802.570681	5.382298	-0.021746	2.382327
111.667351	1810.639603	5.387302	-0.021773	2.387123
112.008698	1818.725477	5.392307	-0.021842	2.391938
112.318560	1826.787384	5.397312	-0.021905	2.396726
112.512742	1834.834644	5.402317	-0.021946	2.401487
112.982179	1842.875798	5.407322	-0.022039	2.406256
113.479477	1850.917296	5.412326	-0.022137	2.411019
113.887721	1858.997749	5.417331	-0.022218	2.415787
114.244843	1867.050728	5.422336	-0.022289	2.420526
114.466952	1875.126315	5.427341	-0.022336	2.425259
114.885391	1883.198123	5.432346	-0.022419	2.429995
114.999490	1891.345088	5.437350	-0.022446	2.434742
115.282404	1899.377918	5.442355	-0.022504	2.439427
115.565630	1907.409621	5.447360	-0.022561	2.444101
115.778878	1915.456875	5.452365	-0.022606	2.448771
116.217621	1923.528854	5.457370	-0.022693	2.453463
116.260409	1931.581769	5.462374	-0.022706	2.458105
116.451388	1939.651815	5.467379	-0.022747	2.462759
116.903252	1947.685590	5.472384	-0.022836	2.467403
117.151926	1955.753582	5.477389	-0.022888	2.472043
117.743144	1963.791338	5.482394	-0.023003	2.476682
118.055869	1971.815759	5.487398	-0.023067	2.481284
118.539352	1979.866926	5.492403	-0.023162	2.485906
118.939560	1987.949377	5.497408	-0.023242	2.490530
119.071417	1996.035758	5.502413	-0.023271	2.495128
119.271902	2004.099343	5.507418	-0.023314	2.499710
119.581559	2012.128165	5.512422	-0.023377	2.504272
119.932597	2020.212753	5.517427	-0.023447	2.508860
120.251847	2028.303965	5.522432	-0.023512	2.513440
120.611823	2036.331296	5.527437	-0.023584	2.517980
121.047827	2044.358617	5.532442	-0.023671	2.522516
121.160392	2052.421599	5.537446	-0.023697	2.527042
121.576995	2060.479361	5.542451	-0.023779	2.531577
121.918776	2068.547930	5.547456	-0.023848	2.536106
121.722705	2076.638918	5.552461	-0.023817	2.540600
122.120045	2084.672492	5.557466	-0.023896	2.545097
122.489757	2092.717556	5.562470	-0.023970	2.549590
122.782548	2100.800872	5.567475	-0.024030	2.554091
122.984481	2108.851092	5.572480	-0.024073	2.558559
123.141517	2116.892043	5.577485	-0.024107	2.563011
123.279573	2124.981207	5.582490	-0.024138	2.567481
123.575893	2133.018117	5.587494	-0.024198	2.571925
123.821438	2141.085727	5.592499	-0.024249	2.576374
124.464663	2149.074038	5.597504	-0.024374	2.580800
124.625638	2157.130795	5.602509	-0.024409	2.585223
125.002993	2165.204157	5.607514	-0.024485	2.589661
125.098582	2173.450435	5.612518	-0.024508	2.594168
125.278599	2181.471156	5.617523	-0.024547	2.598549
125.450792	2189.459386	5.622528	-0.024584	2.602904
125.732239	2197.463954	5.627533	-0.024642	2.607269
126.134295	2205.489941	5.632538	-0.024722	2.611646
126.480374	2213.520686	5.637542	-0.024791	2.616014
126.854104	2221.544302	5.642547	-0.024866	2.620373
127.199314	2229.554029	5.647552	-0.024935	2.624715
127.549615	2237.609691	5.652557	-0.025006	2.629075
127.894583	2245.684831	5.657562	-0.025075	2.633438
128.034513	2253.747497	5.662566	-0.025106	2.637774
128.364444	2261.773700	5.667571	-0.025173	2.642095
128.630071	2269.829585	5.672576	-0.025228	2.646420
128.906703	2277.870261	5.677581	-0.025284	2.650732
129.390800	2285.937004	5.682586	-0.025380	2.655063
129.505127	2293.990603	5.687590	-0.025406	2.659356
129.830052	2302.028756	5.692595	-0.025472	2.663648
130.177546	2310.085581	5.697600	-0.025542	2.667944
130.037462	2318.195206	5.702605	-0.025521	2.672230
130.646759	2326.224776	5.707610	-0.025640	2.676515
131.017956	2334.219979	5.712614	-0.025714	2.680759
131.212711	2342.270098	5.717619	-0.025755	2.685015
131.189733	2350.346254	5.722624	-0.025756	2.689263
131.681510	2358.378079	5.727629	-0.025853	2.693514
132.071430	2366.424387	5.732634	-0.025931	2.697759
132.132534	2374.459749	5.737638	-0.025947	2.701972
132.374010	2382.518391	5.742643	-0.025998	2.706201
132.865359	2390.552779	5.747648	-0.026094	2.710426
133.106148	2398.609480	5.752653	-0.026144	2.714641
133.341729	2406.660859	5.757658	-0.026193	2.718846
133.612870	2414.676131	5.762662	-0.026249	2.723028
133.757847	2422.745346	5.767667	-0.026281	2.727223
134.121568	2430.787914	5.772672	-0.026354	2.731412
134.478643	2438.843228	5.777677	-0.026426	2.735600
134.732954	2446.883903	5.782682	-0.026478	2.739769
134.820487	2454.928148	5.787686	-0.026500	2.743922
134.846281	2463.014351	5.792691	-0.026510	2.748087
135.259485	2471.095924	5.797696	-0.026592	2.752267
135.462837	2479.148890	5.802701	-0.026635	2.756413
135.651898	2487.179202	5.807706	-0.026675	2.760540
135.998787	2495.158036	5.812710	-0.026745	2.764644
136.297077	2503.204732	5.817715	-0.026806	2.768774
136.496496	2511.269619	5.822720	-0.026848	2.772901
136.891691	2519.279737	5.827725	-0.026927	2.777006
137.211797	2527.321090	5.832730	-0.026992	2.781116
137.473855	2535.333891	5.837734	-0.027046	2.785201
137.635943	2543.405899	5.842739	-0.027081	2.789305
138.071096	2551.451587	5.847744	-0.027167	2.793406
138.381932	2559.473020	5.852749	-0.027230	2.797480
138.509821	2567.544081	5.857754	-0.027259	2.801564
138.723369	2575.569453	5.862758	-0.027304	2.805623
139.116841	2583.603940	5.867763	-0.027383	2.809691
139.310675	2591.677498	5.872768	-0.027424	2.813762
139.434000	2599.724249	5.877773	-0.027452	2.817809
139.785881	2607.781504	5.882778	-0.027523	2.821868
139.891439	2615.791865	5.887782	-0.027548	2.825884
140.404861	2623.826076	5.892787	-0.027648	2.829930
140.718936	2631.928493	5.897792	-0.027712	2.833992
140.633493	2639.969512	5.902797	-0.027701	2.837996
141.016088	2647.986498	5.907802	-0.027778	2.842008
141.316550	2655.981562	5.912806	-0.027839	2.845999
141.721202	2664.021600	5.917811	-0.027920	2.850012
141.857082	2672.100284	5.922816	-0.027950	2.854024
142.081257	2680.120537	5.927821	-0.027997	2.858006
142.444737	2688.161145	5.932826	-0.028070	2.862000
142.512145	2696.180491	5.937830	-0.028088	2.865962
142.811123	2704.228849	5.942835	-0.028148	2.869945
143.145885	2712.308057	5.947840	-0.028216	2.873940
143.367003	2720.329986	5.952845	-0.028262	2.877895
143.482111	2728.385041	5.957850	-0.028289	2.881855
143.554210	2736.411399	5.962854	-0.028307	2.885793
143.993580	2744.420233	5.967859	-0.028394	2.889737
144.175149	2752.502620	5.972864	-0.028433	2.893698
144.438568	2760.530837	5.977869	-0.028488	2.897631
144.890501	2768.565376	5.982874	-0.028577	2.901572
145.122753	2776.580048	5.987878	-0.028625	2.905486
145.436785	2784.627533	5.992883	-0.028689	2.909415
145.661185	2792.782122	5.997888	-0.028736	2.913386
145.955677	2800.779853	6.002893	-0.028796	2.917279
146.059456	2808.834411	6.007898	-0.028821	2.921184
146.215803	2816.791355	6.012902	-0.028855	2.925040
146.413357	2824.850156	6.017907	-0.028897	2.928942
146.655545	2832.903960	6.022912	-0.028947	2.932838
146.809570	2840.936649	6.027917	-0.028981	2.936715
147.088471	2848.969134	6.032922	-0.029038	2.940593
147.428032	2856.957050	6.037926	-0.029107	2.944447
147.576459	2865.025064	6.042931	-0.029139	2.948325
147.857606	2873.096683	6.047936	-0.029197	2.952206
148.099632	2881.121903	6.052941	-0.029247	2.956058
148.221538	2889.162101	6.057946	-0.029275	2.959906
148.628110	2897.162741	6.062950	-0.029356	2.963745
148.884449	2905.196574	6.067955	-0.029409	2.967586
149.054233	2913.266595	6.072960	-0.029446	2.971436
148.871076	2921.354492	6.077965	-0.029417	2.975271
149.340935	2929.334695	6.082970	-0.029509	2.979083
149.677703	2937.357273	6.087974	-0.029577	2.982903
149.887308	2945.393877	6.092979	-0.029621	2.986719
150.151872	2953.431770	6.097984	-0.029676	2.990533
150.512371	2961.493112	6.102989	-0.029748	2.994358
151.024416	2969.475499	6.107994	-0.029849	2.998148
150.874512	2977.535120	6.112998	-0.029826	3.001938
151.198537	2985.560492	6.118003	-0.029892	3.005729
151.402330	2993.584818	6.123008	-0.029935	3.009510
151.503664	3001.649352	6.128013	-0.029959	3.013299
151.858851	3009.716305	6.133018	-0.030030	3.017097
151.851210	3017.747938	6.138022	-0.030034	3.020857
152.204225	3025.732086	6.143027	-0.030105	3.024606
152.561396	3033.767384	6.148032	-0.030176	3.028376
152.929283	3041.802400	6.153037	-0.030250	3.032140
153.350617	3049.900437	6.158042	-0.030334	3.035932
153.387020	3057.885972	6.163046	-0.030346	3.039649
153.542846	3065.935590	6.168051	-0.030380	3.043396
153.786963	3073.992214	6.173056	-0.030431	3.047146
153.980180	3082.010188	6.178061	-0.030472	3.050872
154.321794	3090.062712	6.183066	-0.030540	3.054615
154.542091	3098.072138	6.188070	-0.030587	3.058328
154.873423	3106.109876	6.193075	-0.030654	3.062056
154.928163	3114.159288	6.198080	-0.030669	3.065770
155.233463	3122.160523	6.203085	-0.030731	3.069470
155.484753	3130.297229	6.208090	-0.030783	3.073225
155.612039	3138.315833	6.213094	-0.030812	3.076916
156.176136	3146.291905	6.218099	-0.030922	3.080603
156.393753	3154.307260	6.223104	-0.030968	3.084287
156.590524	3162.316672	6.228109	-0.031009	3.087963
157.024874	3170.359729	6.233114	-0.031096	3.091661
157.340658	3178.389633	6.238118	-0.031160	3.095343
157.720446	3186.392745	6.243123	-0.031235	3.099012
157.707022	3194.482448	6.248128	-0.031238	3.102697
157.809650	3202.529040	6.253133	-0.031262	3.106364
158.071892	3210.567976	6.258138	-0.031316	3.110030
158.280259	3218.610181	6.263142	-0.031360	3.113691
158.517906	3226.643914	6.268147	-0.031410	3.117345
158.645489	3234.678756	6.273152	-0.031439	3.120990
159.026626	3242.648374	6.278157	-0.031515	3.124613
159.314640	3250.704338	6.283162	-0.031574	3.128266
159.656905	3258.705726	6.288166	-0.031643	3.131893
159.972121	3266.767025	6.293171	-0.031706	3.135542
159.820874	3274.828667	6.298176	-0.031684	3.139165
160.010640	3282.855878	6.303181	-0.031724	3.142784
160.401804	3290.902043	6.308186	-0.031802	3.146416
160.601292	3298.902544	6.313190	-0.031844	3.150015
160.768543	3307.003933	6.318195	-0.031881	3.153654
160.973983	3315.014096	6.323200	-0.031924	3.157249
161.085557	3323.038372	6.328205	-0.031950	3.160843
161.254811	3331.050200	6.333210	-0.031987	3.164429
161.435965	3339.056764	6.338214	-0.032026	3.168009
161.907279	3347.081785	6.343219	-0.032119	3.171606
162.059648	3355.146002	6.348224	-0.032152	3.175203
162.516788	3363.126394	6.353229	-0.032242	3.178771
162.653065	3371.203555	6.358234	-0.032273	3.182364
162.807777	3379.219871	6.363238	-0.032307	3.185928
162.934949	3387.245042	6.368243	-0.032336	3.189489
163.271072	3395.317313	6.373248	-0.032404	3.193077
163.347177	3403.344309	6.378253	-0.032423	3.196629
163.802559	3411.340237	6.383258	-0.032513	3.200180
163.898658	3419.358588	6.388262	-0.032536	3.203722
163.990002	3427.406868	6.393267	-0.032558	3.207272
164.311044	3435.480183	6.398272	-0.032623	3.210840
164.541024	3443.488761	6.403277	-0.032671	3.214371
164.774826	3451.524400	6.408282	-0.032720	3.217910
165.038914	3459.544827	6.413286	-0.032774	3.221439
165.276261	3467.563132	6.418291	-0.032824	3.224963
165.787698	3475.565607	6.423296	-0.032924	3.228487
165.861779	3483.673309	6.428301	-0.032943	3.232036
166.001213	3491.761756	6.433306	-0.032974	3.235575
166.189274	3499.718632	6.438310	-0.033014	3.239054
166.632438	3507.713719	6.443315	-0.033102	3.242557
166.849642	3515.753492	6.448320	-0.033148	3.246066
167.036233	3523.725880	6.453325	-0.033188	3.249541
167.436835	3531.796618	6.458330	-0.033267	3.253063
167.481925	3539.852602	6.463334	-0.033281	3.256561
167.794427	3547.824477	6.468339	-0.033344	3.260029
168.179776	3555.866910	6.473344	-0.033421	3.263527
168.454806	3563.871121	6.478349	-0.033478	3.267000
168.798674	3571.916078	6.483354	-0.033547	3.270490
168.909250	3579.997373	6.488358	-0.033573	3.273982
169.349851	3588.009824	6.493363	-0.033660	3.277454
169.237254	3596.061850	6.498368	-0.033644	3.280918
169.478965	3604.034668	6.503373	-0.033694	3.284358
169.792739	3612.088735	6.508378	-0.033758	3.287832
169.936336	3620.140483	6.513382	-0.033790	3.291295
170.136294	3628.189940	6.518387	-0.033832	3.294755
170.447846	3636.212529	6.523392	-0.033895	3.298204
170.476680	3644.249771	6.528397	-0.033906	3.301645
170.443246	3652.259287	6.533402	-0.033905	3.305068
170.869037	3660.273849	6.538406	-0.033989	3.308507
171.163134	3668.317350	6.543411	-0.034049	3.311950
171.311671	3676.390961	6.548416	-0.034082	3.315397
171.125465	3684.414374	6.553421	-0.034053	3.318806
171.611475	3692.402554	6.558426	-0.034148	3.322222
171.673568	3700.413418	6.563430	-0.034165	3.325628
172.037509	3708.419483	6.568435	-0.034238	3.329040
172.101345	3716.493915	6.573440	-0.034255	3.332466
172.449630	3724.489345	6.578445	-0.034325	3.335865
172.801906	3732.534836	6.583450	-0.034396	3.339283
172.971582	3740.571997	6.588454	-0.034432	3.342686
173.227546	3748.574500	6.593459	-0.034485	3.346075
173.536566	3756.602159	6.598464	-0.034548	3.349473
173.630107	3764.658822	6.603469	-0.034571	3.352871
173.790399	3772.742487	6.608474	-0.034606	3.356280
174.212318	3780.650958	6.613478	-0.034689	3.359621
174.247251	3788.715695	6.618483	-0.034701	3.363011
174.568031	3796.751658	6.623488	-0.034766	3.366395
174.776099	3804.744334	6.628493	-0.034810	3.369754
175.319613	3812.811431	6.633498	-0.034916	3.373152
175.413575	3820.856181	6.638502	-0.034939	3.376522
175.570934	3828.883507	6.643507	-0.034973	3.379883
175.807576	3836.901029	6.648512	-0.035023	3.383239
175.935192	3844.934269	6.653517	-0.035052	3.386595
176.489305	3852.940650	6.658522	-0.035160	3.389951
176.501099	3861.089728	6.663526	-0.035167	3.393345
176.761982	3869.097843	6.668531	-0.035221	3.396685
177.080406	3877.054320	6.673536	-0.035286	3.400002
177.119870	3885.044830	6.678541	-0.035298	3.403320
177.423796	3893.075549	6.683546	-0.035360	3.406661
177.521035	3901.086098	6.688550	-0.035383	3.409983
177.901046	3909.149187	6.693555	-0.035459	3.413333
178.197910	3917.191700	6.698560	-0.035520	3.416669
178.310288	3925.173379	6.703565	-0.035546	3.419970
178.669165	3933.200236	6.708570	-0.035618	3.423294
178.715557	3941.217327	6.713574	-0.035631	3.426601
178.970699	3949.260122	6.718579	-0.035684	3.429922
179.165194	3957.324864	6.723584	-0.035726	3.433247
179.310261	3965.334651	6.728589	-0.035758	3.436545
179.755633	3973.342445	6.733594	-0.035846	3.439848
180.107575	3981.337499	6.738598	-0.035916	3.443140
179.991110	3989.413012	6.743603	-0.035900	3.446446
180.156875	3997.452285	6.748608	-0.035936	3.449744
180.406240	4005.461357	6.753613	-0.035988	3.453028
180.774457	4013.514568	6.758618	-0.036061	3.456332
180.901225	4021.512993	6.763622	-0.036090	3.459602
181.071876	4029.526293	6.768627	-0.036127	3.462876
181.435487	4037.577996	6.773632	-0.036200	3.466169
181.478383	4045.594548	6.778637	-0.036213	3.469434
181.694468	4053.669557	6.783642	-0.036259	3.472726
181.976055	4061.698005	6.788646	-0.036316	3.475998
182.279229	4069.677842	6.793651	-0.036378	3.479247
182.556315	4077.697357	6.798656	-0.036435	3.482508
182.722791	4085.713098	6.803661	-0.036471	3.485762
183.106791	4093.717973	6.808666	-0.036547	3.489015
183.340178	4101.763796	6.813670	-0.036596	3.492276
183.317750	4109.828524	6.818675	-0.036597	3.495534
183.683573	4117.809723	6.823680	-0.036670	3.498768
183.955087	4125.830513	6.828685	-0.036726	3.502011
184.294936	4133.837354	6.833690	-0.036794	3.505248
184.555449	4141.868691	6.838694	-0.036848	3.508489
184.541084	4149.954184	6.843699	-0.036851	3.511741
184.804600	4157.973166	6.848704	-0.036905	3.514971
184.960381	4165.957261	6.853709	-0.036939	3.518181
185.296405	4174.023856	6.858714	-0.037007	3.521427
185.479798	4181.966941	6.863718	-0.037046	3.524616
185.684183	4190.024172	6.868723	-0.037089	3.527847
186.020375	4198.076648	6.873728	-0.037157	3.531078
186.190141	4206.103018	6.878733	-0.037194	3.534291
186.523756	4214.176947	6.883738	-0.037261	3.537524
186.550409	4222.156015	6.888742	-0.037271	3.540708
186.673225	4230.190782	6.893747	-0.037299	3.543914
186.929881	4238.227671	6.898752	-0.037352	3.547121
186.959405	4246.251066	6.903757	-0.037363	3.550314
187.321885	4254.393895	6.908762	-0.037436	3.553561
187.476648	4262.373196	6.913766	-0.037470	3.556733
187.652174	4270.351879	6.918771	-0.037508	3.559904
187.802436	4278.367190	6.923776	-0.037541	3.563085
188.152339	4286.353090	6.928781	-0.037611	3.566258
188.626913	4294.315092	6.933786	-0.037705	3.569422
188.896744	4302.405119	6.938790	-0.037760	3.572627
189.121788	4310.424326	6.943795	-0.037807	3.575801
189.486110	4318.463671	6.948800	-0.037880	3.578983
189.425130	4326.483913	6.953805	-0.037874	3.582143
189.842984	4334.476053	6.958810	-0.037957	3.585303
189.954809	4342.525919	6.963814	-0.037983	3.588474
190.415325	4350.533447	6.968819	-0.038074	3.591636
190.673327	4358.556302	6.973824	-0.038127	3.594794
190.826206	4366.594598	6.978829	-0.038161	3.597954
191.238972	4374.614468	6.983834	-0.038243	3.601110
191.218517	4382.613161	6.988838	-0.038244	3.604243
191.446926	4390.618047	6.993843	-0.038292	3.607383
191.620549	4398.669002	6.998848	-0.038329	3.610536
191.689667	4406.720011	7.003853	-0.038347	3.613684
191.784970	4414.789850	7.008858	-0.038370	3.616838
191.826990	4422.776010	7.013862	-0.038383	3.619954
192.285894	4430.753759	7.018867	-0.038474	3.623076
192.429650	4438.812556	7.023872	-0.038506	3.626218
192.593756	4446.809576	7.028877	-0.038542	3.629333
192.774035	4454.886355	7.033882	-0.038580	3.632478
193.150503	4462.917352	7.038886	-0.038656	3.635607
193.376293	4470.884465	7.043891	-0.038703	3.638705
193.585743	4478.953842	7.048896	-0.038747	3.641839
193.701486	4486.887490	7.053901	-0.038774	3.644915
194.065607	4494.950648	7.058906	-0.038847	3.648046
194.390091	4502.987242	7.063910	-0.038912	3.651162
194.615716	4511.035099	7.068915	-0.038959	3.654278
194.739750	4519.107283	7.073920	-0.038988	3.657397
194.825166	4527.090225	7.078925	-0.039009	3.660479
195.191890	4535.105701	7.083930	-0.039082	3.663577
195.393200	4543.154574	7.088934	-0.039125	3.666682
195.383602	4551.176490	7.093939	-0.039128	3.669768
195.727636	4559.233723	7.098944	-0.039198	3.672874
196.160055	4567.226231	7.103949	-0.039283	3.675955
196.113847	4575.228691	7.108954	-0.039280	3.679024
196.135791	4583.258597	7.113958	-0.039289	3.682104
196.609925	4591.215083	7.118963	-0.039382	3.685164
196.625079	4599.294857	7.123968	-0.039390	3.688257
196.813555	4607.308900	7.128973	-0.039431	3.691327
197.152139	4615.347751	7.133978	-0.039499	3.694408
197.624083	4623.327582	7.138982	-0.039592	3.697466
197.818750	4631.328032	7.143987	-0.039633	3.700524
198.038288	4639.374560	7.148992	-0.039679	3.703596
198.408651	4647.379663	7.153997	-0.039754	3.706654
198.629272	4655.427383	7.159002	-0.039800	3.709722
198.982430	4663.505461	7.164006	-0.039871	3.712802
199.286496	4671.559825	7.169011	-0.039933	3.715870
199.205985	4679.561418	7.174016	-0.039923	3.718905
199.393744	4687.544350	7.179021	-0.039963	3.721938
199.951976	4695.500677	7.184026	-0.040072	3.724966
200.161040	4703.526879	7.189030	-0.040116	3.728011
200.284229	4711.575019	7.194035	-0.040144	3.731059
200.412586	4719.617087	7.199040	-0.040173	3.734102
200.729515	4727.611893	7.204045	-0.040237	3.737129
200.743813	4735.647799	7.209050	-0.040245	3.740163
200.800798	4743.710795	7.214054	-0.040261	3.743205
201.197524	4751.684044	7.219059	-0.040340	3.746218
201.376731	4759.767661	7.224064	-0.040379	3.749266
201.471034	4767.790077	7.229069	-0.040401	3.752286
201.824238	4775.824823	7.234074	-0.040472	3.755315
201.940052	4783.861520	7.239078	-0.040499	3.758336
201.919003	4791.850615	7.244083	-0.040500	3.761334
202.295738	4799.827893	7.249088	-0.040576	3.764334
202.256625	4807.891750	7.254093	-0.040574	3.767354
202.602069	4815.883106	7.259098	-0.040643	3.770354
202.729773	4823.958292	7.264102	-0.040672	3.773377
203.078741	4831.975863	7.269107	-0.040742	3.776382
203.399137	4839.930595	7.274112	-0.040807	3.779360
203.473225	4847.987512	7.279117	-0.040826	3.782368
203.797204	4855.962430	7.284122	-0.040891	3.785349
203.948101	4864.031920	7.289126	-0.040925	3.788359
204.190348	4872.061440	7.294131	-0.040975	3.791354
204.848395	4880.081530	7.299136	-0.041103	3.794352
205.423940	4888.098778	7.304141	-0.041215	3.797344
205.246512	4896.140227	7.309146	-0.041187	3.800327
205.342251	4904.160346	7.314150	-0.041210	3.803305
205.553964	4912.144743	7.319155	-0.041255	3.806270
205.798347	4920.132746	7.324160	-0.041305	3.809235
205.767438	4928.236480	7.329165	-0.041305	3.812235
205.939063	4936.252302	7.334170	-0.041342	3.815204
206.167115	4944.231533	7.339174	-0.041390	3.818158
206.615709	4952.262056	7.344179	-0.041478	3.821134
206.811594	4960.225299	7.349184	-0.041520	3.824077
206.922989	4968.259650	7.354189	-0.041546	3.827042
207.283627	4976.292250	7.359194	-0.041618	3.830010
207.504529	4984.334808	7.364198	-0.041665	3.832976
207.519321	4992.349333	7.369203	-0.041672	3.835925
208.008065	5000.349698	7.374208	-0.041769	3.838876
208.126753	5008.407498	7.379213	-0.041796	3.841838
208.307845	5016.412835	7.384218	-0.041835	3.844781
208.867077	5024.416412	7.389222	-0.041944	3.847728
208.982063	5032.386753	7.394227	-0.041971	3.850651
208.770531	5040.557531	7.399232	-0.041936	3.853639
209.129094	5048.543164	7.404237	-0.042008	3.856568
209.561474	5056.494311	7.409242	-0.042094	3.859484
209.456258	5064.566970	7.414246	-0.042080	3.862432
209.638167	5072.563616	7.419251	-0.042119	3.865355
209.889428	5080.674839	7.424256	-0.042171	3.868319
209.723953	5088.703235	7.429261	-0.042145	3.871242
209.821635	5096.976595	7.434266	-0.042169	3.874258
210.006762	5104.925757	7.439270	-0.042208	3.877155
210.552077	5112.706539	7.444275	-0.042315	3.879995
210.955646	5120.726713	7.449280	-0.042395	3.882918
211.231989	5128.670326	7.454285	-0.042452	3.885808
211.543483	5136.709377	7.459290	-0.042515	3.888731
211.845672	5144.783525	7.464294	-0.042576	3.891664
212.008826	5152.805586	7.469299	-0.042612	3.894574
212.118053	5160.852892	7.474304	-0.042637	3.897490
212.071166	5168.851275	7.479309	-0.042634	3.900383
212.274312	5176.839341	7.484314	-0.042677	3.903274
212.423089	5184.904494	7.489318	-0.042710	3.906190
212.463371	5192.889540	7.494323	-0.042722	3.909074
212.901264	5200.915819	7.499328	-0.042809	3.911977
213.029419	5208.922262	7.504333	-0.042838	3.914865
213.316822	5216.965713	7.509338	-0.042897	3.917767
213.664011	5224.937642	7.514342	-0.042967	3.920643
213.799273	5232.941759	7.519347	-0.042997	3.923524
214.023105	5241.011744	7.524352	-0.043044	3.926428
214.043718	5249.010000	7.529357	-0.043053	3.929300
214.477928	5257.078209	7.534362	-0.043139	3.932203
214.562054	5265.096558	7.539366	-0.043160	3.935080
214.727893	5273.054944	7.544371	-0.043196	3.937934
214.847055	5281.130485	7.549376	-0.043223	3.940828
214.818349	5289.132756	7.554381	-0.043223	3.943690
215.214272	5297.151818	7.559386	-0.043302	3.946564
215.396191	5305.141716	7.564390	-0.043341	3.949421
215.517260	5313.207757	7.569395	-0.043369	3.952303
215.672582	5321.263230	7.574400	-0.043403	3.955179
215.945825	5329.216544	7.579405	-0.043459	3.958019
216.213546	5337.202256	7.584410	-0.043514	3.960868
216.290439	5345.236152	7.589414	-0.043533	3.963729
216.602879	5353.263108	7.594419	-0.043597	3.966590
216.793946	5361.274419	7.599424	-0.043637	3.969440
216.987171	5369.297633	7.604429	-0.043678	3.972293
217.219163	5377.375069	7.609434	-0.043727	3.975164
217.418572	5385.360444	7.614438	-0.043769	3.977999
217.417822	5393.384576	7.619443	-0.043774	3.980843
217.765164	5401.425021	7.624448	-0.043844	3.983696
217.892860	5409.442538	7.629453	-0.043873	3.986536
218.070582	5417.456504	7.634458	-0.043911	3.989373
218.258273	5425.489064	7.639462	-0.043951	3.992214
218.440905	5433.537390	7.644467	-0.043991	3.995060
218.753473	5441.550334	7.649472	-0.044054	3.997892
218.767068	5449.532798	7.654477	-0.044062	4.000707
219.006949	5457.556966	7.659482	-0.044111	4.003539
219.003037	5465.638466	7.664486	-0.044116	4.006384
219.179158	5473.600663	7.669491	-0.044154	4.009189
219.727405	5481.673943	7.674496	-0.044261	4.012036
219.735824	5489.705565	7.679501	-0.044268	4.014858
219.782611	5497.733183	7.684506	-0.044282	4.017678
220.038989	5505.714715	7.689510	-0.044335	4.020482
220.427203	5513.672231	7.694515	-0.044412	4.023278
220.611279	5521.749344	7.699520	-0.044452	4.026111
220.532795	5529.744384	7.704525	-0.044442	4.028910
221.187240	5537.775540	7.709530	-0.044569	4.031729
221.383423	5545.904248	7.714534	-0.044611	4.034574
221.346275	5553.885883	7.719539	-0.044609	4.037363
221.547029	5561.861315	7.724544	-0.044652	4.040150
221.729994	5569.814443	7.729549	-0.044691	4.042928
221.996765	5577.843109	7.734554	-0.044746	4.045731
222.104260	5585.846367	7.739558	-0.044771	4.048521
222.177398	5593.875440	7.744563	-0.044790	4.051318
222.301034	5601.952922	7.749568	-0.044818	4.054130
222.465319	5609.950891	7.754573	-0.044854	4.056914
223.013877	5617.912864	7.759578	-0.044961	4.059688
223.250477	5625.938913	7.764582	-0.045010	4.062478
223.298962	5633.930397	7.769587	-0.045024	4.065252
223.585366	5642.016085	7.774592	-0.045083	4.068059
223.639104	5650.011235	7.779597	-0.045098	4.070830
223.747584	5658.047590	7.784602	-0.045123	4.073614
223.854778	5666.099473	7.789606	-0.045149	4.076402
223.909848	5674.058700	7.794611	-0.045164	4.079155
224.110631	5682.108063	7.799616	-0.045206	4.081939
224.204429	5690.027863	7.804621	-0.045229	4.084675
224.466656	5698.112172	7.809626	-0.045283	4.087469
224.991005	5706.097030	7.814630	-0.045386	4.090229
224.943551	5714.156351	7.819635	-0.045382	4.093006
225.220211	5722.188935	7.824640	-0.045439	4.095776
225.474055	5730.183471	7.829645	-0.045491	4.098530
225.673555	5738.172816	7.834650	-0.045534	4.101280
225.813736	5746.216165	7.839654	-0.045565	4.104046
225.904791	5754.275918	7.844659	-0.045587	4.106816
225.982812	5762.347096	7.849664	-0.045607	4.109587
226.151733	5770.323003	7.854669	-0.045643	4.112324
226.533975	5778.354852	7.859674	-0.045720	4.115082
226.799125	5786.360024	7.864678	-0.045774	4.117827
226.881586	5794.352599	7.869683	-0.045795	4.120564
227.145938	5802.361362	7.874688	-0.045849	4.123307
227.275670	5810.343824	7.879693	-0.045879	4.126037
227.581187	5818.372948	7.884698	-0.045941	4.128783
227.670249	5826.448114	7.889702	-0.045962	4.131541
227.745803	5834.467856	7.894707	-0.045982	4.134278
228.265051	5842.555362	7.899712	-0.046084	4.137041
228.297350	5850.485692	7.904717	-0.046095	4.139743
228.478997	5858.516067	7.909722	-0.046134	4.142479
228.676681	5866.522828	7.914726	-0.046176	4.145206
228.827234	5874.552170	7.919731	-0.046209	4.147937
229.036999	5882.580275	7.924736	-0.046253	4.150668
229.313964	5890.638172	7.929741	-0.046310	4.153407
229.581542	5898.645683	7.934746	-0.046365	4.156127
229.626048	5906.643875	7.939750	-0.046378	4.158840
229.815696	5914.656338	7.944755	-0.046419	4.161557
230.065438	5922.692438	7.949760	-0.046470	4.164281
230.113497	5930.693438	7.954765	-0.046485	4.166990
230.307447	5938.696779	7.959770	-0.046526	4.169699
230.502507	5946.757121	7.964774	-0.046567	4.172425
230.607455	5954.754519	7.969779	-0.046592	4.175128
230.773648	5962.791280	7.974784	-0.046628	4.177842
230.727778	5970.787293	7.979789	-0.046625	4.180539
231.005832	5978.788446	7.984794	-0.046682	4.183239
231.022383	5986.809565	7.989798	-0.046690	4.185942
230.999778	5994.842665	7.994803	-0.046691	4.188646
231.215591	6002.871729	7.999808	-0.046736	4.191350
231.493796	6010.964531	8.004813	-0.046793	4.194073
231.618323	6018.981900	8.009818	-0.046822	4.196769
232.010629	6026.915449	8.014822	-0.046900	4.199437
232.287830	6034.928407	8.019827	-0.046957	4.202129
232.396584	6042.916279	8.024832	-0.046982	4.204808
232.412175	6050.912068	8.029837	-0.046990	4.207488
232.960619	6058.891637	8.034842	-0.047097	4.210166
232.854983	6067.009538	8.039846	-0.047083	4.212883
232.930875	6075.030255	8.044851	-0.047102	4.215566
233.389377	6083.010480	8.049856	-0.047193	4.218238
233.405733	6091.012411	8.054861	-0.047201	4.220912
233.473006	6099.040426	8.059866	-0.047219	4.223593
233.803571	6107.068918	8.064870	-0.047285	4.226274
234.180948	6115.031089	8.069875	-0.047361	4.228933
234.213296	6123.097115	8.074880	-0.047372	4.231621
234.522580	6131.142783	8.079885	-0.047435	4.234303
234.721108	6139.155450	8.084890	-0.047477	4.236971
234.917106	6147.134827	8.089894	-0.047519	4.239627
234.894316	6155.183495	8.094899	-0.047519	4.242302
235.219720	6163.181777	8.099904	-0.047585	4.244961
235.686427	6171.183314	8.104909	-0.047677	4.247622
235.941927	6179.183442	8.109914	-0.047730	4.250278
236.242635	6187.231767	8.114918	-0.047791	4.252949
236.597194	6195.261251	8.119923	-0.047862	4.255612
236.759919	6203.300903	8.124928	-0.047898	4.258276
236.943022	6211.281903	8.129933	-0.047937	4.260918
237.116839	6219.363561	8.134938	-0.047975	4.263592
237.243738	6227.376908	8.139942	-0.048003	4.266241
237.381403	6235.353421	8.144947	-0.048034	4.268877
237.544337	6243.408094	8.149952	-0.048070	4.271537
237.602771	6251.439212	8.154957	-0.048086	4.274187
237.930248	6259.503774	8.159962	-0.048152	4.276848
238.182650	6267.423664	8.164966	-0.048204	4.279459
238.438311	6275.460347	8.169971	-0.048257	4.282107
238.541989	6283.424144	8.174976	-0.048281	4.284728
238.591805	6291.507165	8.179981	-0.048296	4.287387
238.838632	6299.500298	8.184986	-0.048347	4.290015
239.069619	6307.520682	8.189990	-0.048395	4.292651
239.160753	6315.550299	8.194995	-0.048417	4.295288
239.612779	6323.599427	8.200000	-0.048507	4.297931
239.781139	6331.593498	8.205005	-0.048543	4.300553
239.859609	6339.573588	8.210010	-0.048563	4.303168
239.931937	6347.624522	8.215014	-0.048582	4.305805
239.904655	6355.646379	8.220019	-0.048582	4.308429
240.233317	6363.627070	8.225024	-0.048648	4.311041
240.260885	6371.704372	8.230029	-0.048658	4.313681
240.503564	6379.707400	8.235034	-0.048709	4.316297
240.777988	6387.712792	8.240038	-0.048765	4.318912
240.827567	6395.758574	8.245043	-0.048779	4.321537
241.143352	6403.735652	8.250048	-0.048843	4.324140
241.064861	6411.740282	8.255053	-0.048834	4.326747
241.187989	6419.753219	8.260058	-0.048862	4.329357
241.266621	6427.784435	8.265062	-0.048882	4.331971
241.575082	6435.788030	8.270067	-0.048944	4.334576
241.866871	6443.817085	8.275072	-0.049004	4.337188
241.944202	6451.808264	8.280077	-0.049023	4.339784
242.054388	6459.866149	8.285082	-0.049049	4.342401
242.183446	6467.846759	8.290086	-0.049078	4.344991
242.389285	6475.866344	8.295091	-0.049122	4.347592
242.802694	6483.915767	8.300096	-0.049204	4.350203
242.813133	6491.999041	8.305101	-0.049211	4.352821
242.848296	6500.031731	8.310106	-0.049223	4.355421
242.920488	6508.024143	8.315110	-0.049241	4.358007
242.964638	6515.966788	8.320115	-0.049255	4.360575
243.310177	6524.028535	8.325120	-0.049324	4.363181
243.504789	6531.984794	8.330125	-0.049366	4.365751
243.939143	6540.000608	8.335130	-0.049452	4.368340
244.085752	6548.026409	8.340134	-0.049484	4.370929
243.884569	6556.047567	8.345139	-0.049452	4.373513
244.223205	6564.090312	8.350144	-0.049520	4.376106
244.515037	6572.062126	8.355149	-0.049580	4.378674
244.525952	6580.106547	8.360154	-0.049587	4.381262
244.777300	6588.095421	8.365158	-0.049639	4.383832
245.001353	6596.128412	8.370163	-0.049686	4.386414
245.171639	6604.148628	8.375168	-0.049723	4.388991
245.173930	6612.187020	8.380173	-0.049728	4.391571
245.541459	6620.223411	8.385178	-0.049802	4.394151
245.723954	6628.265616	8.390182	-0.049841	4.396730
245.756922	6636.192109	8.395187	-0.049852	4.399270
246.011587	6644.273931	8.400192	-0.049905	4.401859
246.194135	6652.188974	8.405197	-0.049944	4.404393
246.300715	6660.259174	8.410202	-0.049969	4.406974
246.635564	6668.231168	8.415206	-0.050036	4.409524
246.825082	6676.325367	8.420211	-0.050077	4.412110
247.297143	6684.384194	8.425216	-0.050170	4.414685
247.058963	6692.399148	8.430221	-0.050131	4.417242
247.152333	6700.366092	8.435226	-0.050153	4.419783
247.520015	6708.388803	8.440230	-0.050227	4.422341
247.494264	6716.354925	8.445235	-0.050227	4.424878
247.917474	6724.433476	8.450240	-0.050311	4.427452
248.024052	6732.444466	8.455245	-0.050336	4.430001
248.094483	6740.528353	8.460250	-0.050355	4.432572
248.115174	6748.519324	8.465254	-0.050364	4.435111
248.381011	6756.507909	8.470259	-0.050418	4.437649
248.691158	6764.478993	8.475264	-0.050481	4.440181
248.596291	6772.573830	8.480269	-0.050469	4.442748
248.466945	6780.549618	8.485274	-0.050450	4.445276
248.929482	6788.567355	8.490278	-0.050541	4.447819
249.031648	6796.528916	8.495283	-0.050565	4.450340
249.160166	6804.648668	8.500288	-0.050595	4.452911
249.529161	6812.587866	8.505293	-0.050668	4.455423
249.878118	6820.638603	8.510298	-0.050739	4.457970
249.951564	6828.616969	8.515302	-0.050757	4.460491
250.120140	6836.616690	8.520307	-0.050794	4.463017
250.374694	6844.662686	8.525312	-0.050846	4.465557
250.378746	6852.692135	8.530317	-0.050852	4.468090
250.477554	6860.669735	8.535322	-0.050876	4.470605
250.804121	6868.762668	8.540326	-0.050942	4.473156
250.812386	6876.763207	8.545331	-0.050949	4.475675
251.039366	6884.768217	8.550336	-0.050996	4.478194
251.487487	6892.743054	8.555341	-0.051085	4.480704
251.655453	6900.759813	8.560346	-0.051121	4.483224
251.514725	6908.783845	8.565351	-0.051100	4.485745
251.610584	6916.773528	8.570355	-0.051123	4.488254
251.975471	6924.861028	8.575360	-0.051196	4.490792
252.146365	6932.872185	8.580365	-0.051233	4.493305
252.333874	6940.911683	8.585370	-0.051273	4.495826
252.732124	6948.838508	8.590375	-0.051353	4.498310
252.740091	6956.804736	8.595379	-0.051359	4.500804
252.977971	6964.891471	8.600384	-0.051409	4.503335
253.327239	6972.943119	8.605389	-0.051479	4.505854
253.381855	6980.949509	8.610394	-0.051494	4.508356
253.335298	6988.992049	8.615399	-0.051491	4.510869
253.449534	6997.023005	8.620403	-0.051517	4.513376
254.029222	7005.065536	8.625408	-0.051630	4.515887
254.074174	7013.040965	8.630413	-0.051644	4.518374
254.091572	7020.999938	8.635418	-0.051652	4.520855
254.417212	7029.005631	8.640423	-0.051718	4.523350
254.568728	7037.021863	8.645427	-0.051751	4.525846
255.102463	7045.049571	8.650432	-0.051856	4.528344
255.032067	7053.068987	8.655437	-0.051848	4.530838
255.135561	7061.092941	8.660442	-0.051872	4.533332
255.550166	7069.114851	8.665447	-0.051955	4.535825
255.515471	7077.114233	8.670451	-0.051954	4.538309
255.844511	7085.136525	8.675456	-0.052020	4.540798
256.058356	7093.136652	8.680461	-0.052065	4.543280
256.226533	7101.123292	8.685466	-0.052101	4.545756
256.317338	7109.209411	8.690471	-0.052124	4.548261
256.366523	7117.188224	8.695475	-0.052138	4.550731
256.632872	7125.225157	8.700480	-0.052193	4.553218
256.639526	7133.274498	8.705485	-0.052199	4.555708
257.091551	7141.249121	8.710490	-0.052288	4.558173
256.981281	7149.276326	8.715495	-0.052273	4.560653
257.140240	7157.261647	8.720499	-0.052308	4.563119
257.368493	7165.262322	8.725504	-0.052355	4.565588
257.448152	7173.314330	8.730509	-0.052375	4.568072
257.624039	7181.298639	8.735514	-0.052413	4.570533
257.746763	7189.412098	8.740519	-0.052441	4.573033
257.951557	7197.385909	8.745523	-0.052485	4.575488
258.192105	7205.444202	8.750528	-0.052535	4.577968
258.242463	7213.372173	8.755533	-0.052549	4.580407
258.552605	7221.427038	8.760538	-0.052612	4.582883
258.909794	7229.416221	8.765543	-0.052684	4.585338
259.037124	7237.426253	8.770547	-0.052713	4.587798
259.191895	7245.507782	8.775552	-0.052747	4.590278
259.388363	7253.532659	8.780557	-0.052788	4.592740
259.348008	7261.554810	8.785562	-0.052786	4.595200
259.536906	7269.579244	8.790567	-0.052826	4.597659
259.633378	7277.535629	8.795571	-0.052850	4.600095
259.759217	7285.567709	8.800576	-0.052878	4.602554
259.879880	7293.521454	8.805581	-0.052906	4.604987
260.161196	7301.533739	8.810586	-0.052963	4.607437
260.286151	7309.585996	8.815591	-0.052992	4.609898
260.351621	7317.642534	8.820595	-0.053009	4.612358
260.727281	7325.698763	8.825600	-0.053084	4.614818
261.024165	7333.664124	8.830605	-0.053145	4.617248
261.145250	7341.617085	8.835610	-0.053172	4.619673
261.268648	7349.717728	8.840615	-0.053201	4.622142
261.446394	7357.619904	8.845619	-0.053239	4.624549
261.566100	7365.749729	8.850624	-0.053266	4.627024
261.785339	7373.698481	8.855629	-0.053312	4.629443
262.013030	7381.739810	8.860634	-0.053360	4.631888
262.187107	7389.777102	8.865639	-0.053397	4.634331
261.915584	7397.775104	8.870643	-0.053352	4.636761
262.344961	7405.768330	8.875648	-0.053437	4.639188
262.302455	7413.813573	8.880653	-0.053434	4.641630
262.366398	7421.774918	8.885658	-0.053451	4.644045
262.707867	7429.846632	8.890663	-0.053520	4.646491
263.031851	7437.846404	8.895667	-0.053586	4.648915
263.006329	7445.904608	8.900672	-0.053586	4.651355
263.152078	7453.854354	8.905677	-0.053618	4.653762
263.515484	7461.878493	8.910682	-0.053691	4.656189
263.890387	7469.903929	8.915687	-0.053766	4.658615
263.714055	7477.890511	8.920691	-0.053739	4.661029
263.989832	7485.980815	8.925696	-0.053795	4.663472
264.016865	7493.918915	8.930701	-0.053805	4.665868
264.074568	7501.986520	8.935706	-0.053821	4.668303
264.280764	7509.994027	8.940711	-0.053865	4.670717
264.537378	7518.057881	8.945715	-0.053918	4.673147
264.810206	7526.107487	8.950720	-0.053974	4.675572
264.661676	7534.077700	8.955725	-0.053951	4.677972
264.856756	7542.020057	8.960730	-0.053993	4.680362
265.405136	7550.055204	8.965735	-0.054100	4.682778
265.293511	7558.020368	8.970739	-0.054084	4.685173
265.509901	7566.079298	8.975744	-0.054130	4.687594
265.844423	7574.055003	8.980749	-0.054197	4.689988
266.202521	7582.128736	8.985754	-0.054269	4.692411
266.211985	7590.206082	8.990759	-0.054276	4.694834
266.550470	7598.194499	8.995763	-0.054344	4.697229
266.588243	7606.155433	9.000768	-0.054356	4.699615
266.724227	7614.200507	9.005773	-0.054387	4.702024
266.813121	7622.151310	9.010778	-0.054409	4.704404
267.144808	7630.196022	9.015783	-0.054476	4.706811
266.990800	7638.189368	9.020787	-0.054452	4.709202
267.241110	7646.235435	9.025792	-0.054504	4.711607
267.372000	7654.268896	9.030797	-0.054533	4.714007
267.649344	7662.300621	9.035802	-0.054590	4.716404
267.961047	7670.276208	9.040807	-0.054653	4.718784
268.001758	7678.251102	9.045811	-0.054666	4.721163
268.137174	7686.308524	9.050816	-0.054697	4.723565
267.941363	7694.314221	9.055821	-0.054665	4.725951
268.314539	7702.309043	9.060826	-0.054740	4.728332
268.766444	7710.392823	9.065831	-0.054829	4.730737
268.648526	7718.396890	9.070835	-0.054812	4.733119
269.086256	7726.443802	9.075840	-0.054899	4.735511
269.274072	7734.440601	9.080845	-0.054939	4.737887
269.561852	7742.424800	9.085850	-0.054998	4.740258
269.617906	7750.507098	9.090855	-0.055014	4.742658
269.586984	7758.438853	9.095859	-0.055013	4.745012
269.485363	7766.562098	9.100864	-0.054999	4.747423
269.773057	7774.503686	9.105869	-0.055058	4.749776
270.032633	7782.484800	9.110874	-0.055111	4.752141
270.251710	7790.591767	9.115879	-0.055158	4.754541
270.268230	7798.562092	9.120883	-0.055166	4.756901
270.608670	7806.545974	9.125888	-0.055234	4.759262
270.820738	7814.537506	9.130893	-0.055279	4.761625
271.005355	7822.527438	9.135898	-0.055318	4.763986
270.952587	7830.600555	9.140903	-0.055314	4.766371
271.032667	7838.562199	9.145907	-0.055334	4.768722
271.449520	7846.668042	9.150912	-0.055417	4.771113
271.645161	7854.644720	9.155917	-0.055458	4.773465
271.597708	7862.681153	9.160922	-0.055455	4.775835
271.794670	7870.707191	9.165927	-0.055496	4.778200
271.941335	7878.657024	9.170931	-0.055529	4.780541
272.315674	7886.701265	9.175936	-0.055604	4.782908
272.451874	7894.654701	9.180941	-0.055634	4.785248
272.594998	7902.748092	9.185946	-0.055666	4.787628
272.556366	7910.734346	9.190951	-0.055664	4.789976
272.722682	7918.773499	9.195955	-0.055700	4.792337
273.268112	7926.798398	9.200960	-0.055807	4.794692
273.092378	7934.891123	9.205965	-0.055779	4.797068
273.130789	7942.722096	9.210970	-0.055792	4.799366
273.365024	7950.877460	9.215975	-0.055841	4.801756
273.428942	7958.741110	9.220979	-0.055858	4.804061
273.640992	7966.834954	9.225984	-0.055902	4.806431
273.903273	7974.836716	9.230989	-0.055956	4.808773
274.036187	7982.860478	9.235994	-0.055986	4.811120
274.161174	7990.447219	9.240999	-0.056014	4.813339
274.253980	7995.154827	9.246003	-0.056035	4.814715

274.472755	7997.764272	9.251008	-0.056077	4.815477
274.616500	7999.078320	9.256013	-0.056105	4.815861
274.597780	7999.534025	9.261018	-0.056101	4.815994
274.844161	8000.289319	9.266023	-0.056148	4.816213
274.831158	8000.488814	9.271027	-0.056145	4.816272
274.791218	8000.503041	9.276032	-0.056138	4.816276
274.779097	8000.502816	9.281037	-0.056135	4.816276
274.894155	8000.559363	9.286042	-0.056157	4.816292
274.863682	8000.495789	9.291047	-0.056151	4.816274
274.848419	8000.488031	9.296051	-0.056148	4.816271
275.168116	8000.393398	9.301056	-0.056208	4.816242
275.275360	8000.504278	9.306061	-0.056228	4.816274
275.188179	8000.407635	9.311066	-0.056211	4.816246
275.286934	8000.383779	9.316071	-0.056230	4.816239
275.436759	8000.611854	9.321075	-0.056258	4.816305
275.541719	8000.506933	9.326080	-0.056277	4.816273
275.536616	8000.477996	9.331085	-0.056276	4.816265
275.607933	8000.539094	9.336090	-0.056289	4.816282
275.541525	8000.442825	9.341095	-0.056277	4.816255
275.489179	8000.498485	9.346099	-0.056267	4.816271
275.570618	8000.519177	9.351104	-0.056282	4.816277
275.505518	8000.595969	9.356109	-0.056270	4.816300
275.651969	8000.492865	9.361114	-0.056297	4.816269
275.911396	8000.409961	9.366119	-0.056345	4.816243
275.648926	8000.514162	9.371123	-0.056296	4.816275
275.902134	8000.501642	9.376128	-0.056344	4.816270
275.865800	8000.480686	9.381133	-0.056337	4.816264
275.836132	8000.508984	9.386138	-0.056331	4.816272
275.815259	8000.434900	9.391143	-0.056327	4.816251
275.889128	8000.575087	9.396147	-0.056341	4.816291
276.333372	8000.420753	9.401152	-0.056424	4.816244
276.230967	8000.407147	9.406157	-0.056404	4.816241
276.126949	8000.494986	9.411162	-0.056385	4.816267
276.382510	8000.408807	9.416167	-0.056432	4.816240
276.306482	8000.516379	9.421171	-0.056418	4.816272
276.397801	8000.401596	9.426176	-0.056435	4.816238
276.158848	8000.358819	9.431181	-0.056391	4.816227
276.212531	8000.525346	9.436186	-0.056401	4.816275
276.334035	8000.274387	9.441191	-0.056423	4.816201
276.243689	8000.542989	9.446195	-0.056406	4.816280
276.375373	8000.355234	9.451200	-0.056431	4.816225
276.217525	8000.515801	9.456205	-0.056401	4.816272
276.306618	8000.513134	9.461210	-0.056418	4.816271
276.533138	8000.400794	9.466215	-0.056460	4.816237
276.491580	8000.397902	9.471219	-0.056452	4.816237
276.550248	8000.495090	9.476224	-0.056463	4.816265
276.493597	8000.433176	9.481229	-0.056452	4.816247
276.528133	8000.411364	9.486234	-0.056459	4.816240
276.455158	8000.410040	9.491239	-0.056445	4.816240
276.297434	8000.527884	9.496243	-0.056416	4.816276
276.514744	8000.494421	9.501248	-0.056456	4.816265
276.638626	8000.522291	9.506253	-0.056479	4.816272
276.615642	8000.512257	9.511258	-0.056475	4.816269
276.591270	8000.547060	9.516263	-0.056470	4.816280
276.644058	8000.557622	9.521267	-0.056480	4.816282
276.781707	8000.506697	9.526272	-0.056506	4.816267
276.791147	8000.506862	9.531277	-0.056507	4.816267
276.806096	8000.512468	9.536282	-0.056510	4.816268
276.587392	8000.417716	9.541287	-0.056469	4.816242
276.595081	8000.543892	9.546291	-0.056471	4.816279
276.766891	8000.336566	9.551296	-0.056503	4.816217
276.651826	8000.511794	9.556301	-0.056481	4.816269
276.542142	8000.511942	9.561306	-0.056461	4.816270
276.721438	8000.516246	9.566311	-0.056494	4.816270
276.724515	8000.522706	9.571315	-0.056495	4.816272
276.825748	8000.367511	9.576320	-0.056513	4.816226
276.830304	8000.378270	9.581325	-0.056514	4.816229
276.836050	8000.423231	9.586330	-0.056515	4.816242
277.013291	8000.363408	9.591335	-0.056548	4.816224
276.732928	8000.422424	9.596339	-0.056496	4.816242
276.851174	8000.346581	9.601344	-0.056518	4.816220
276.810822	8000.411003	9.606349	-0.056510	4.816239
276.798847	8000.354170	9.611354	-0.056508	4.816222
276.918620	8000.388374	9.616359	-0.056530	4.816232
276.767022	8000.507398	9.621363	-0.056502	4.816267
276.825865	8000.404845	9.626368	-0.056513	4.816237
276.859900	8000.496248	9.631373	-0.056519	4.816263
276.892842	8000.525679	9.636378	-0.056525	4.816272
276.889669	8000.424141	9.641383	-0.056524	4.816242
276.918341	8000.318907	9.646387	-0.056530	4.816211
277.098078	8000.406534	9.651392	-0.056563	4.816236
277.072976	8000.335577	9.656397	-0.056558	4.816215
277.068857	8000.354724	9.661402	-0.056558	4.816221
276.975116	8000.410704	9.666407	-0.056540	4.816238
276.950893	8000.410261	9.671411	-0.056535	4.816238
277.031666	8000.404239	9.676416	-0.056550	4.816236
276.811619	8000.289168	9.681421	-0.056509	4.816203
276.780058	8000.386862	9.686426	-0.056503	4.816232
276.896904	8000.381492	9.691431	-0.056525	4.816230
276.862842	8000.415052	9.696435	-0.056519	4.816240
276.968615	8000.399868	9.701440	-0.056538	4.816235
276.911336	8000.390282	9.706445	-0.056528	4.816232
276.806270	8000.380900	9.711450	-0.056508	4.816230
276.924336	8000.416142	9.716455	-0.056530	4.816240
277.014219	8000.494669	9.721459	-0.056547	4.816262
277.006623	8000.406937	9.726464	-0.056545	4.816237
277.126018	8000.489202	9.731469	-0.056567	4.816260
277.155558	8000.397868	9.736474	-0.056573	4.816233
277.139025	8000.191411	9.741479	-0.056570	4.816173
277.071829	8000.342936	9.746483	-0.056557	4.816217
277.201503	8000.212824	9.751488	-0.056581	4.816179
277.243147	8000.390885	9.756493	-0.056589	4.816231
277.227165	8000.423704	9.761498	-0.056586	4.816240
277.096609	8000.324136	9.766503	-0.056562	4.816212
276.788085	8000.382643	9.771507	-0.056504	4.816231
277.144870	8000.216046	9.776512	-0.056570	4.816180
276.952641	8000.364244	9.781517	-0.056535	4.816224
277.021555	8000.370825	9.786522	-0.056547	4.816226
277.261499	8000.285431	9.791527	-0.056592	4.816200
277.205533	8000.357049	9.796531	-0.056581	4.816221
277.218214	8000.344455	9.801536	-0.056584	4.816217
277.462747	8000.332848	9.806541	-0.056629	4.816212
277.096407	8000.450127	9.811546	-0.056561	4.816249
277.216329	8000.277111	9.816551	-0.056583	4.816197
277.214111	8000.419131	9.821555	-0.056583	4.816239
277.395902	8000.189553	9.826560	-0.056616	4.816171
277.186533	8000.406872	9.831565	-0.056578	4.816236
276.989939	8000.290088	9.836570	-0.056541	4.816202
277.274695	8000.320865	9.841575	-0.056594	4.816210
277.311735	8000.317257	9.846579	-0.056601	4.816209
277.297104	8000.360782	9.851584	-0.056598	4.816222
277.101087	8000.266440	9.856589	-0.056561	4.816195
277.330183	8000.406232	9.861594	-0.056604	4.816235
277.432890	8000.278835	9.866599	-0.056623	4.816197
277.306414	8000.420746	9.871603	-0.056599	4.816239
277.242615	8000.357634	9.876608	-0.056588	4.816221
277.280474	8000.239747	9.881613	-0.056594	4.816186
277.048396	8000.343431	9.886618	-0.056551	4.816218
277.326924	8000.192509	9.891623	-0.056603	4.816172
277.344470	8000.219525	9.896627	-0.056606	4.816180
277.375728	8000.273492	9.901632	-0.056612	4.816196
277.610549	8000.132462	9.906637	-0.056656	4.816153
277.607568	8000.215719	9.911642	-0.056655	4.816178
277.509063	8000.263068	9.916647	-0.056637	4.816192
277.353980	8000.187625	9.921651	-0.056608	4.816171
277.478883	8000.148219	9.926656	-0.056631	4.816158
277.469076	8000.258057	9.931661	-0.056629	4.816191
277.425292	8000.240169	9.936666	-0.056621	4.816186
277.453439	8000.037724	9.941671	-0.056626	4.816126
277.515431	8000.420171	9.946675	-0.056638	4.816238
277.408137	8000.089234	9.951680	-0.056617	4.816142
277.491490	8000.274457	9.956685	-0.056633	4.816195
277.433865	8000.116392	9.961690	-0.056622	4.816149
277.406028	8000.213085	9.966695	-0.056617	4.816178
277.563651	8000.204179	9.971699	-0.056646	4.816174
277.521648	8000.283526	9.976704	-0.056638	4.816198
277.406736	8000.242990	9.981709	-0.056617	4.816187
277.354861	8000.268751	9.986714	-0.056607	4.816194
277.466681	8000.224836	9.991719	-0.056628	4.816181
277.420483	8000.260313	9.996723	-0.056619	4.816192
277.496631	8000.228571	10.001728	-0.056633	4.816182
277.617668	8000.260662	10.006733	-0.056656	4.816191
277.632097	8000.242759	10.011738	-0.056658	4.816185
277.544901	8000.225155	10.016743	-0.056642	4.816181
277.353098	8000.378702	10.021747	-0.056606	4.816227
277.364671	8000.353270	10.026752	-0.056609	4.816219
277.456575	8000.400857	10.031757	-0.056626	4.816232
277.221978	8000.415837	10.036762	-0.056582	4.816238
277.400206	8000.260966	10.041767	-0.056615	4.816192
277.652635	8000.433226	10.046771	-0.056662	4.816241
277.591051	8000.163998	10.051776	-0.056650	4.816163
277.575361	8000.210708	10.056781	-0.056647	4.816176
277.559536	8000.251007	10.061786	-0.056644	4.816188
277.532173	8000.197099	10.066791	-0.056639	4.816173
277.435307	8000.247682	10.071795	-0.056621	4.816188
277.427726	8000.095862	10.076800	-0.056620	4.816143
277.746355	8000.261840	10.081805	-0.056679	4.816190
277.568713	8000.351553	10.086810	-0.056646	4.816217
277.467535	8000.226880	10.091815	-0.056627	4.816182
277.583682	8000.167021	10.096819	-0.056648	4.816163
277.507788	8000.206234	10.101824	-0.056634	4.816175
277.466840	8000.193739	10.106829	-0.056627	4.816172
277.635979	8000.292925	10.111834	-0.056658	4.816200
277.873333	8000.236325	10.116839	-0.056702	4.816182
277.652198	8000.327389	10.121843	-0.056661	4.816210
277.670054	8000.235844	10.126848	-0.056664	4.816183
277.846704	8000.359735	10.131853	-0.056697	4.816218
277.830774	8000.257966	10.136858	-0.056694	4.816189
277.754251	8000.334553	10.141863	-0.056680	4.816212
277.620777	8000.290476	10.146867	-0.056655	4.816199
277.627406	8000.180570	10.151872	-0.056656	4.816167
277.621087	8000.199677	10.156877	-0.056655	4.816173
277.760960	8000.247063	10.161882	-0.056681	4.816186
277.748368	8000.224399	10.166887	-0.056678	4.816179
277.701134	8000.331424	10.171891	-0.056670	4.816211
278.020387	8000.371373	10.176896	-0.056729	4.816221
277.999464	8000.206490	10.181901	-0.056725	4.816173
277.732634	8000.164276	10.186906	-0.056675	4.816162
277.578659	8000.146533	10.191911	-0.056646	4.816158
277.676427	8000.412132	10.196915	-0.056665	4.816235
277.598571	8000.136201	10.201920	-0.056650	4.816154
277.675442	8000.287127	10.206925	-0.056664	4.816198
277.752645	8000.342994	10.211930	-0.056679	4.816214
278.135249	8000.172590	10.216935	-0.056750	4.816162
277.978359	8000.298997	10.221939	-0.056721	4.816200
277.899912	8000.049759	10.226944	-0.056706	4.816128
277.922604	8000.126003	10.231949	-0.056710	4.816150
277.841201	8000.182207	10.236954	-0.056695	4.816167
277.851816	8000.198416	10.241959	-0.056697	4.816171
277.842955	8000.127752	10.246963	-0.056695	4.816151
277.876773	8000.116608	10.251968	-0.056701	4.816147
277.615227	8000.196260	10.256973	-0.056653	4.816172
277.532534	8000.224668	10.261978	-0.056637	4.816181
277.823071	8000.197869	10.266983	-0.056691	4.816171
277.730255	8000.304071	10.271987	-0.056674	4.816203
277.827030	8000.149863	10.276992	-0.056692	4.816157
277.616594	8000.237916	10.281997	-0.056653	4.816184
277.459198	8000.216907	10.287002	-0.056623	4.816179
277.701931	8000.188176	10.292007	-0.056668	4.816169
277.525210	8000.291792	10.297011	-0.056635	4.816200
277.963889	8000.148037	10.302016	-0.056717	4.816156
278.021901	8000.207830	10.307021	-0.056728	4.816173
277.836861	8000.300614	10.312026	-0.056693	4.816201
277.893309	8000.290948	10.317031	-0.056704	4.816198
278.003692	8000.305756	10.322035	-0.056724	4.816202
277.902489	8000.278285	10.327040	-0.056705	4.816194
278.024787	8000.301854	10.332045	-0.056728	4.816201
277.812843	8000.259563	10.337050	-0.056689	4.816189
278.120813	8000.319602	10.342055	-0.056746	4.816205
277.915526	8000.298795	10.347059	-0.056708	4.816200
277.976894	8000.163173	10.352064	-0.056719	4.816160
277.905701	8000.274038	10.357069	-0.056706	4.816193
277.709875	8000.252334	10.362074	-0.056669	4.816188
277.965837	8000.253751	10.367079	-0.056717	4.816187
277.929291	8000.420789	10.372083	-0.056710	4.816236
277.993818	8000.206179	10.377088	-0.056722	4.816173
278.000736	8000.275730	10.382093	-0.056723	4.816193
278.199862	8000.377597	10.387098	-0.056760	4.816222
278.123751	8000.232011	10.392103	-0.056746	4.816180
278.051292	8000.240310	10.397107	-0.056732	4.816182
277.998369	8000.295961	10.402112	-0.056722	4.816199
278.113759	8000.227542	10.407117	-0.056744	4.816178
277.900299	8000.184155	10.412122	-0.056704	4.816167
278.032511	7999.980385	10.417127	-0.056728	4.816107
277.989633	8000.219941	10.422131	-0.056720	4.816177
277.748247	8000.258298	10.427136	-0.056676	4.816189
277.799126	8000.170555	10.432141	-0.056685	4.816163
277.894600	8000.141299	10.437146	-0.056703	4.816154
277.873576	8000.102460	10.442151	-0.056699	4.816143
277.891568	8000.181824	10.447155	-0.056702	4.816166
278.180013	8000.146442	10.452160	-0.056756	4.816154
278.306193	8000.056855	10.457165	-0.056779	4.816128
277.992142	8000.339579	10.462170	-0.056721	4.816212
278.253504	8000.197959	10.467175	-0.056769	4.816169
277.974870	8000.264483	10.472179	-0.056717	4.816190
277.989530	8000.172881	10.477184	-0.056720	4.816163
278.084210	8000.213041	10.482189	-0.056737	4.816174
277.754328	8000.078893	10.487194	-0.056676	4.816137
278.147265	8000.047536	10.492199	-0.056749	4.816126
277.974941	8000.167255	10.497203	-0.056717	4.816162
278.170381	8000.251963	10.502208	-0.056753	4.816185
278.089798	8000.081731	10.507213	-0.056738	4.816136
277.995144	8000.293648	10.512218	-0.056721	4.816198
278.248833	8000.128389	10.517223	-0.056768	4.816149
278.297302	8000.040602	10.522227	-0.056777	4.816123
278.141588	8000.160621	10.527232	-0.056748	4.816159
278.173044	8000.098163	10.532237	-0.056753	4.816140
278.135891	8000.236348	10.537242	-0.056746	4.816181
278.114815	8000.025533	10.542247	-0.056742	4.816119
277.959860	8000.130611	10.547251	-0.056713	4.816151
277.879422	8000.000973	10.552256	-0.056698	4.816114
278.005819	8000.013933	10.557261	-0.056722	4.816117
277.886746	8000.159181	10.562266	-0.056700	4.816160
277.942624	7999.997826	10.567271	-0.056710	4.816112
278.085151	8000.050600	10.572275	-0.056736	4.816127
277.900316	7999.994914	10.577280	-0.056702	4.816112
277.930171	8000.000789	10.582285	-0.056707	4.816113
277.887835	8000.003223	10.587290	-0.056700	4.816114
278.062265	7999.997825	10.592295	-0.056732	4.816112
277.897995	8000.084576	10.597299	-0.056701	4.816138
278.030963	8000.031430	10.602304	-0.056726	4.816122
278.094271	8000.172498	10.607309	-0.056738	4.816163
277.961059	8000.255538	10.612314	-0.056713	4.816187
278.210198	8000.147879	10.617319	-0.056759	4.816155
278.109818	8000.244330	10.622323	-0.056741	4.816183
278.055447	8000.212365	10.627328	-0.056730	4.816174
278.120513	8000.165468	10.632333	-0.056742	4.816160
278.165795	8000.352144	10.637338	-0.056751	4.816215
278.129524	8000.133576	10.642343	-0.056744	4.816151
277.998681	8000.205977	10.647347	-0.056720	4.816173
278.084083	8000.082540	10.652352	-0.056735	4.816136
278.271530	8000.198081	10.657357	-0.056770	4.816169
278.084776	8000.249176	10.662362	-0.056736	4.816185
277.993553	8000.214408	10.667367	-0.056718	4.816175
278.232513	8000.208041	10.672371	-0.056763	4.816172
278.188986	8000.094023	10.677376	-0.056755	4.816139
278.073980	7999.923169	10.682381	-0.056733	4.816090
277.980880	8000.207748	10.687386	-0.056716	4.816173
278.137761	8000.036468	10.692391	-0.056745	4.816123
278.151932	8000.174512	10.697395	-0.056748	4.816163
278.278613	8000.001617	10.702400	-0.056771	4.816112
278.246550	8000.167666	10.707405	-0.056765	4.816160
278.190749	8000.132471	10.712410	-0.056755	4.816150
278.205506	8000.043006	10.717415	-0.056757	4.816124
278.199670	8000.230893	10.722419	-0.056756	4.816179
278.163374	8000.064665	10.727424	-0.056749	4.816131
278.278435	8000.150057	10.732429	-0.056771	4.816155
278.189742	8000.148448	10.737434	-0.056754	4.816155
278.299893	8000.064981	10.742439	-0.056775	4.816130
278.128004	8000.300070	10.747443	-0.056743	4.816200
278.405338	8000.003854	10.752448	-0.056794	4.816112
278.329216	8000.212902	10.757453	-0.056780	4.816173
278.331841	8000.034560	10.762458	-0.056780	4.816121
278.256946	8000.095154	10.767463	-0.056766	4.816139
278.325845	8000.203212	10.772467	-0.056779	4.816170
278.371927	8000.131404	10.777472	-0.056788	4.816149
278.391722	8000.196915	10.782477	-0.056791	4.816168
278.231815	8000.271995	10.787482	-0.056762	4.816191
278.382833	8000.069631	10.792487	-0.056789	4.816131
278.151911	8000.247040	10.797491	-0.056747	4.816184
278.253649	8000.074762	10.802496	-0.056765	4.816133
278.388840	8000.030201	10.807501	-0.056790	4.816119
278.400054	8000.234419	10.812506	-0.056793	4.816179
278.280827	8000.034647	10.817511	-0.056770	4.816121
278.155698	8000.150946	10.822515	-0.056747	4.816156
278.243414	8000.137572	10.827520	-0.056763	4.816152
278.502979	8000.045055	10.832525	-0.056811	4.816123
278.263020	8000.312028	10.837530	-0.056767	4.816202
278.359630	8000.062749	10.842535	-0.056785	4.816129
278.411850	8000.243140	10.847539	-0.056794	4.816182
278.337756	8000.194796	10.852544	-0.056781	4.816168
278.423327	8000.150406	10.857549	-0.056796	4.816154
278.335828	8000.286613	10.862554	-0.056780	4.816195
278.482033	8000.059594	10.867559	-0.056807	4.816128
278.330510	8000.194643	10.872563	-0.056779	4.816168
278.500015	8000.181680	10.877568	-0.056810	4.816163
278.365466	8000.115151	10.882573	-0.056785	4.816144
278.093115	7999.995930	10.887578	-0.056734	4.816111
278.519457	8000.128606	10.892583	-0.056814	4.816148
278.405466	8000.124404	10.897587	-0.056793	4.816147
278.435646	8000.089694	10.902592	-0.056798	4.816137
278.342484	8000.010029	10.907597	-0.056781	4.816114
278.381639	8000.225434	10.912602	-0.056788	4.816177
278.352199	8000.068943	10.917607	-0.056782	4.816131
278.290763	8000.273984	10.922611	-0.056771	4.816191
278.240511	8000.105367	10.927616	-0.056762	4.816142
278.100060	7999.973575	10.932621	-0.056735	4.816104
278.106739	8000.216164	10.937626	-0.056737	4.816175
277.955866	7999.970959	10.942631	-0.056708	4.816104
278.173259	8000.168220	10.947635	-0.056749	4.816161
278.252798	8000.312788	10.952640	-0.056764	4.816203
278.221774	8000.092178	10.957645	-0.056758	4.816138
278.383747	8000.330100	10.962650	-0.056788	4.816207
278.394698	8000.010908	10.967655	-0.056790	4.816114
278.213509	8000.223397	10.972659	-0.056756	4.816177
278.269107	8000.134671	10.977664	-0.056766	4.816151
278.405721	8000.185203	10.982669	-0.056792	4.816165
278.174619	8000.219474	10.987674	-0.056749	4.816176
278.118537	8000.084933	10.992679	-0.056738	4.816137
278.314296	8000.265783	10.997683	-0.056775	4.816189
278.221938	8000.128450	11.002688	-0.056757	4.816149
278.311473	8000.179199	11.007693	-0.056774	4.816163
278.286906	8000.194772	11.012698	-0.056769	4.816168
278.359950	7999.994204	11.017703	-0.056783	4.816109
278.402256	8000.185097	11.022707	-0.056791	4.816165
278.398459	8000.000230	11.027712	-0.056790	4.816111
278.323456	8000.121708	11.032717	-0.056776	4.816147
278.494638	8000.228411	11.037722	-0.056808	4.816177
278.576564	8000.013047	11.042727	-0.056823	4.816114
278.567733	8000.105813	11.047731	-0.056821	4.816141
278.358802	8000.243029	11.052736	-0.056782	4.816182
278.375588	8000.127964	11.057741	-0.056785	4.816148
278.571334	8000.020408	11.062746	-0.056822	4.816116
278.582545	8000.195786	11.067751	-0.056824	4.816167
278.277251	8000.244738	11.072755	-0.056767	4.816183
278.252938	8000.172725	11.077760	-0.056762	4.816162
278.669459	8000.132182	11.082765	-0.056840	4.816148
278.400188	8000.188195	11.087770	-0.056790	4.816166
278.538216	8000.163980	11.092775	-0.056815	4.816158
278.476971	8000.254731	11.097779	-0.056804	4.816185
278.252720	8000.060537	11.102784	-0.056762	4.816129
278.187070	8000.107412	11.107789	-0.056750	4.816143
278.118316	8000.007893	11.112794	-0.056737	4.816114
278.116513	8000.001446	11.117799	-0.056736	4.816113
277.843901	8000.039240	11.122803	-0.056685	4.816125
278.234350	8000.127472	11.127808	-0.056758	4.816149
278.249002	8000.015574	11.132813	-0.056761	4.816116
278.216183	8000.128201	11.137818	-0.056755	4.816149
278.507702	8000.158034	11.142823	-0.056809	4.816156
278.359067	8000.119024	11.147827	-0.056781	4.816146
278.255887	7999.990041	11.152832	-0.056762	4.816109
278.554485	7999.987956	11.157837	-0.056817	4.816106
278.553500	8000.174863	11.162842	-0.056817	4.816161
278.667093	7999.961140	11.167847	-0.056838	4.816098
278.557447	8000.212310	11.172851	-0.056818	4.816172
278.696878	7999.996918	11.177856	-0.056844	4.816108
278.814848	8000.231909	11.182861	-0.056866	4.816176
278.705482	8000.193607	11.187866	-0.056845	4.816166
278.808462	8000.010669	11.192871	-0.056864	4.816112
278.691937	8000.108965	11.197875	-0.056843	4.816141
278.478956	7999.973725	11.202880	-0.056803	4.816103
278.709196	8000.055858	11.207885	-0.056846	4.816125
278.460651	8000.073791	11.212890	-0.056799	4.816132
278.488545	8000.086039	11.217895	-0.056804	4.816135
278.481590	8000.114749	11.222899	-0.056803	4.816144
278.462382	8000.111192	11.227904	-0.056800	4.816143
278.529705	8000.115608	11.232909	-0.056812	4.816144
278.378511	8000.246391	11.237914	-0.056784	4.816183
278.256083	8000.010243	11.242919	-0.056761	4.816114
278.376119	8000.156610	11.247923	-0.056783	4.816157
278.442985	8000.014679	11.252928	-0.056796	4.816115
278.303182	8000.012147	11.257933	-0.056769	4.816115
278.278159	8000.120642	11.262938	-0.056765	4.816147
278.364699	7999.979067	11.267943	-0.056781	4.816105
278.340656	8000.211487	11.272947	-0.056776	4.816173
278.405419	8000.041746	11.277952	-0.056788	4.816123
278.485029	8000.083770	11.282957	-0.056803	4.816135
278.409434	8000.149693	11.287962	-0.056789	4.816154
278.457311	7999.924101	11.292967	-0.056798	4.816088
278.279427	8000.090719	11.297971	-0.056765	4.816138
278.269174	8000.006143	11.302976	-0.056763	4.816113
278.188303	8000.030312	11.307981	-0.056748	4.816121
278.116252	8000.011913	11.312986	-0.056734	4.816116
278.271956	8000.087357	11.317991	-0.056763	4.816137
278.077208	8000.057128	11.322995	-0.056727	4.816129
278.348738	8000.109030	11.328000	-0.056777	4.816143
278.569536	8000.179243	11.333005	-0.056818	4.816162
278.722703	8000.216189	11.338010	-0.056847	4.816172
278.694958	8000.181500	11.343015	-0.056842	4.816162
278.599746	8000.216092	11.348019	-0.056824	4.816173
278.512078	8000.101274	11.353024	-0.056807	4.816140
278.445312	8000.062676	11.358029	-0.056795	4.816129
278.595200	8000.242698	11.363034	-0.056823	4.816181
278.562249	7999.929122	11.368039	-0.056816	4.816089
278.574563	8000.110928	11.373043	-0.056819	4.816142
278.510780	8000.125792	11.378048	-0.056807	4.816147
278.571838	8000.101254	11.383053	-0.056818	4.816139
278.459075	8000.195346	11.388058	-0.056797	4.816168
278.420264	8000.133753	11.393063	-0.056790	4.816150
278.463311	8000.389821	11.398067	-0.056798	4.816224
278.476511	8000.183895	11.403072	-0.056800	4.816164
278.470188	8000.151730	11.408077	-0.056799	4.816155
278.297767	8000.261834	11.413082	-0.056767	4.816188
278.602788	8000.258799	11.418087	-0.056824	4.816185
278.526744	8000.161282	11.423091	-0.056809	4.816157
278.381421	7999.909767	11.428096	-0.056782	4.816084
278.588518	8000.009639	11.433101	-0.056821	4.816113
278.289448	8000.121726	11.438106	-0.056765	4.816147
278.411379	7999.883588	11.443111	-0.056787	4.816077
278.215557	8000.032790	11.448115	-0.056751	4.816121
278.465759	7999.980695	11.453120	-0.056798	4.816105
278.468894	8000.075813	11.458125	-0.056798	4.816133
278.208538	8000.212099	11.463130	-0.056750	4.816174
278.327808	7999.903414	11.468135	-0.056772	4.816083
278.397460	8000.021097	11.473139	-0.056785	4.816117
278.345989	8000.163296	11.478144	-0.056775	4.816159
278.358412	8000.209446	11.483149	-0.056777	4.816172
278.536790	8000.161394	11.488154	-0.056811	4.816157
278.605419	8000.032312	11.493159	-0.056823	4.816119
278.420165	8000.073821	11.498163	-0.056789	4.816132
278.679278	8000.103068	11.503168	-0.056837	4.816139
278.780653	8000.041873	11.508173	-0.056856	4.816121
278.488028	8000.355963	11.513178	-0.056801	4.816214
278.665448	8000.132711	11.518183	-0.056834	4.816148
278.840036	8000.389023	11.523187	-0.056867	4.816222
278.580185	8000.216613	11.528192	-0.056818	4.816173
278.613381	8000.083685	11.533197	-0.056824	4.816134
278.588918	8000.091783	11.538202	-0.056820	4.816137
278.494975	8000.093284	11.543207	-0.056802	4.816138
278.517592	8000.168459	11.548211	-0.056806	4.816159
278.732447	8000.177680	11.553216	-0.056846	4.816161
278.640469	8000.261466	11.558221	-0.056829	4.816186
278.525571	8000.164315	11.563226	-0.056808	4.816158
278.763611	8000.144045	11.568231	-0.056852	4.816151
278.774140	8000.192299	11.573235	-0.056854	4.816165
278.682277	8000.153246	11.578240	-0.056837	4.816154
278.714523	8000.194414	11.583245	-0.056843	4.816166
278.810072	8000.270910	11.588250	-0.056860	4.816188
278.787176	7999.913719	11.593255	-0.056856	4.816084
278.646540	8000.074601	11.598259	-0.056830	4.816131
278.547143	8000.032208	11.603264	-0.056811	4.816119
278.648339	7999.999851	11.608269	-0.056830	4.816109
278.559781	8000.131766	11.613274	-0.056813	4.816148
278.689519	7999.938631	11.618279	-0.056837	4.816091
278.616144	8000.066548	11.623283	-0.056824	4.816129
278.545048	7999.992621	11.628288	-0.056810	4.816108
278.641913	8000.022139	11.633293	-0.056828	4.816116
278.644113	8000.264650	11.638298	-0.056829	4.816187
278.717307	8000.185855	11.643303	-0.056842	4.816163
278.531256	8000.125872	11.648307	-0.056808	4.816147
278.727893	8000.040763	11.653312	-0.056844	4.816121
278.913566	8000.146660	11.658317	-0.056879	4.816151
278.837725	8000.148488	11.663322	-0.056865	4.816152
278.862639	7999.971615	11.668327	-0.056869	4.816100
278.903212	8000.133638	11.673331	-0.056877	4.816147
278.885868	8000.129047	11.678336	-0.056873	4.816146
278.773848	8000.130220	11.683341	-0.056852	4.816147
279.003494	8000.150390	11.688346	-0.056895	4.816152
279.047771	7999.965322	11.693351	-0.056903	4.816097
278.697127	8000.141635	11.698355	-0.056838	4.816151
278.706963	8000.110831	11.703360	-0.056840	4.816142
278.871566	8000.136233	11.708365	-0.056870	4.816148
278.672375	8000.050377	11.713370	-0.056833	4.816124
278.635657	8000.064662	11.718375	-0.056826	4.816128
278.746602	8000.225821	11.723379	-0.056847	4.816175
278.740249	8000.187246	11.728384	-0.056846	4.816164
278.810124	8000.166073	11.733389	-0.056859	4.816157
278.846337	8000.226541	11.738394	-0.056865	4.816175
278.685588	8000.085833	11.743399	-0.056835	4.816134
278.476757	8000.141870	11.748403	-0.056796	4.816152
278.575809	8000.175701	11.753408	-0.056815	4.816161
278.708826	8000.220828	11.758413	-0.056840	4.816174
278.602951	8000.090727	11.763418	-0.056820	4.816136
278.682658	8000.202185	11.768423	-0.056835	4.816168
278.744102	8000.007814	11.773427	-0.056846	4.816111
278.763051	8000.112832	11.778432	-0.056849	4.816142
278.831815	8000.012593	11.783437	-0.056862	4.816112
278.802095	8000.115664	11.788442	-0.056857	4.816143
278.992205	7999.956733	11.793447	-0.056892	4.816095
278.908550	8000.012896	11.798451	-0.056876	4.816112
278.845462	8000.016023	11.803456	-0.056864	4.816113
278.884377	8000.030607	11.808461	-0.056872	4.816117
278.854709	8000.133679	11.813466	-0.056866	4.816148
278.802137	7999.991724	11.818471	-0.056856	4.816106
278.816162	8000.208812	11.823475	-0.056859	4.816170
278.784084	8000.237068	11.828480	-0.056853	4.816178
278.956939	8000.202802	11.833485	-0.056885	4.816167
278.906594	8000.068363	11.838490	-0.056875	4.816128
278.933649	8000.028256	11.843495	-0.056880	4.816116
278.796066	8000.057809	11.848499	-0.056855	4.816126
278.657393	7999.986933	11.853504	-0.056829	4.816106
279.074064	7999.978438	11.858509	-0.056906	4.816101
278.768153	8000.203629	11.863514	-0.056849	4.816168
278.785342	7999.988162	11.868519	-0.056852	4.816105
278.794955	8000.193421	11.873523	-0.056854	4.816165
278.774451	8000.058454	11.878528	-0.056850	4.816126
278.683917	8000.081380	11.883533	-0.056834	4.816133
278.619726	8000.055646	11.888538	-0.056821	4.816126
278.735760	8000.095124	11.893543	-0.056843	4.816137
278.706239	8000.283654	11.898547	-0.056838	4.816192
278.798755	8000.111207	11.903552	-0.056855	4.816141
278.920137	8000.254397	11.908557	-0.056877	4.816182
278.803960	8000.171109	11.913562	-0.056856	4.816159
278.598262	8000.118248	11.918567	-0.056817	4.816144
278.651255	8000.107451	11.923571	-0.056827	4.816141
278.896155	8000.140714	11.928576	-0.056873	4.816149
278.795104	8000.017109	11.933581	-0.056854	4.816114
279.023032	8000.168634	11.938586	-0.056896	4.816157
279.165958	7999.972531	11.943591	-0.056923	4.816099
279.052959	8000.059141	11.948595	-0.056901	4.816125
278.868615	8000.155144	11.953600	-0.056867	4.816154
279.041904	8000.131567	11.958605	-0.056899	4.816146
278.788573	8000.431415	11.963610	-0.056852	4.816235
278.867493	8000.101698	11.968615	-0.056867	4.816138
278.874171	8000.134927	11.973619	-0.056868	4.816148
278.790792	8000.171869	11.978624	-0.056852	4.816159
278.935036	8000.123199	11.983629	-0.056879	4.816144
278.608501	8000.432404	11.988634	-0.056819	4.816236
278.882153	8000.260028	11.993639	-0.056869	4.816184
278.809383	8000.117706	11.998643	-0.056856	4.816143
278.822188	8000.286706	12.003648	-0.056858	4.816192
279.135517	8000.252844	12.008653	-0.056916	4.816181
278.923059	8000.154996	12.013658	-0.056877	4.816153
278.830115	8000.103105	12.018663	-0.056859	4.816139
278.945386	8000.218412	12.023667	-0.056881	4.816172
279.231496	8000.139193	12.028672	-0.056934	4.816147
279.202501	8000.064958	12.033677	-0.056928	4.816126
279.145933	8000.196386	12.038682	-0.056918	4.816164
279.153685	8000.080088	12.043687	-0.056919	4.816130
279.145217	8000.016906	12.048691	-0.056918	4.816112
278.918292	8000.077957	12.053696	-0.056875	4.816131
278.937687	8000.070825	12.058701	-0.056879	4.816129
279.063151	8000.020747	12.063706	-0.056902	4.816114
278.849669	8000.051064	12.068711	-0.056862	4.816123
278.663963	8000.132087	12.073715	-0.056828	4.816148
278.948565	8000.199183	12.078720	-0.056881	4.816166
278.944308	8000.190555	12.083725	-0.056880	4.816164
278.685059	8000.190134	12.088730	-0.056832	4.816165
278.983808	8000.115417	12.093735	-0.056887	4.816142
279.051865	8000.291826	12.098739	-0.056900	4.816193
279.041567	8000.152769	12.103744	-0.056898	4.816152
278.975481	7999.987069	12.108749	-0.056885	4.816104
278.862284	8000.122812	12.113754	-0.056864	4.816144
278.755174	8000.016189	12.118759	-0.056844	4.816114
278.941143	8000.217159	12.123763	-0.056879	4.816172
279.100876	8000.076905	12.128768	-0.056908	4.816130
278.896132	8000.133016	12.133773	-0.056870	4.816147
278.622637	8000.138747	12.138778	-0.056819	4.816150
278.684279	7999.992449	12.143783	-0.056831	4.816107
278.868200	8000.179495	12.148787	-0.056865	4.816161
278.906206	8000.139586	12.153792	-0.056872	4.816149
278.878760	7999.937199	12.158797	-0.056867	4.816090
278.882348	8000.232076	12.163802	-0.056867	4.816176
278.891622	8000.129692	12.168807	-0.056869	4.816146
278.859911	8000.038318	12.173811	-0.056863	4.816120
278.801617	8000.041532	12.178816	-0.056852	4.816121
278.782738	7999.929027	12.183821	-0.056848	4.816088
278.842962	7999.978178	12.188826	-0.056860	4.816102
279.094411	8000.123719	12.193831	-0.056907	4.816143
279.160567	8000.169774	12.198835	-0.056919	4.816157
278.926434	8000.164466	12.203840	-0.056875	4.816156
278.944728	7999.985337	12.208845	-0.056878	4.816104
278.835931	8000.076296	12.213850	-0.056858	4.816131
279.020480	7999.911924	12.218855	-0.056892	4.816082
278.832083	7999.998239	12.223859	-0.056857	4.816108
279.007108	8000.092193	12.228864	-0.056890	4.816135
279.109337	8000.026741	12.233869	-0.056909	4.816115
279.004316	8000.079314	12.238874	-0.056889	4.816131
278.925982	8000.044779	12.243879	-0.056875	4.816121
279.017148	8000.085944	12.248883	-0.056892	4.816133
279.254327	8000.034682	12.253888	-0.056936	4.816117
279.283975	8000.002099	12.258893	-0.056941	4.816107
279.123800	8000.139129	12.263898	-0.056911	4.816148
279.252729	7999.944909	12.268903	-0.056935	4.816090
279.233705	8000.053515	12.273907	-0.056932	4.816122
279.165913	8000.023443	12.278912	-0.056919	4.816114
279.329359	7999.952688	12.283917	-0.056949	4.816092
279.090186	8000.085085	12.288922	-0.056905	4.816132
279.141121	8000.033660	12.293927	-0.056914	4.816117
279.113421	8000.053449	12.298931	-0.056909	4.816123
279.098464	7999.988014	12.303936	-0.056906	4.816104
279.064713	8000.000217	12.308941	-0.056900	4.816108
279.060902	8000.058893	12.313946	-0.056899	4.816125
279.099147	8000.055306	12.318951	-0.056906	4.816123
279.149337	8000.096799	12.323955	-0.056915	4.816135
279.212832	8000.139601	12.328960	-0.056927	4.816148
279.433768	7999.878681	12.333965	-0.056968	4.816070
279.374473	8000.190583	12.338970	-0.056957	4.816162
279.191864	7999.992865	12.343975	-0.056923	4.816105
279.141086	8000.214124	12.348979	-0.056914	4.816170
279.067688	8000.064313	12.353984	-0.056900	4.816126
279.230910	8000.154851	12.358989	-0.056930	4.816152
279.123120	8000.167851	12.363994	-0.056910	4.816156
279.366305	8000.032310	12.368999	-0.056955	4.816115
279.234286	8000.021372	12.374003	-0.056931	4.816113
279.195041	7999.964044	12.379008	-0.056923	4.816096
279.259883	7999.996188	12.384013	-0.056935	4.816105
279.209965	7999.979257	12.389018	-0.056926	4.816101
279.138633	8000.054871	12.394023	-0.056913	4.816123
279.141925	8000.202335	12.399027	-0.056913	4.816166
279.134864	8000.126361	12.404032	-0.056912	4.816144
279.195339	8000.096472	12.409037	-0.056923	4.816135
279.137884	8000.159519	12.414042	-0.056912	4.816154
279.300566	8000.015045	12.419047	-0.056942	4.816111
279.439171	7999.983364	12.424051	-0.056968	4.816101
279.232712	7999.975353	12.429056	-0.056930	4.816099
279.335831	7999.917394	12.434061	-0.056949	4.816082
279.254093	8000.129547	12.439066	-0.056934	4.816144
279.453982	7999.946224	12.444071	-0.056971	4.816090
279.353167	7999.934782	12.449075	-0.056952	4.816087
279.351897	8000.068277	12.454080	-0.056952	4.816126
279.259338	8000.123212	12.459085	-0.056934	4.816143
279.145953	8000.117951	12.464090	-0.056913	4.816142
279.250655	8000.004475	12.469095	-0.056933	4.816108
278.993461	8000.030797	12.474099	-0.056885	4.816117
278.990109	7999.973049	12.479104	-0.056884	4.816100
279.464285	7999.889753	12.484109	-0.056972	4.816073
279.250698	7999.979886	12.489114	-0.056932	4.816101
279.060579	7999.974307	12.494119	-0.056897	4.816100
279.185614	7999.979767	12.499123	-0.056920	4.816101
279.133387	7999.941431	12.504128	-0.056910	4.816090
279.471393	7999.952878	12.509133	-0.056973	4.816092
279.346171	8000.073450	12.514138	-0.056950	4.816128
279.414418	7999.963587	12.519143	-0.056962	4.816095
279.477123	7999.887806	12.524147	-0.056974	4.816073
279.345790	8000.002926	12.529152	-0.056950	4.816107
279.191650	8000.002270	12.534157	-0.056921	4.816108
279.288819	8000.117250	12.539162	-0.056939	4.816141
279.427252	8000.089838	12.544167	-0.056965	4.816132
279.375702	8000.149788	12.549171	-0.056955	4.816150
279.394367	8000.126620	12.554176	-0.056958	4.816143
279.201751	8000.010971	12.559181	-0.056922	4.816110
279.174004	8000.179238	12.564186	-0.056917	4.816159
279.331663	7999.942810	12.569191	-0.056946	4.816089
279.190817	8000.081258	12.574195	-0.056920	4.816131
279.056561	8000.118348	12.579200	-0.056895	4.816142
279.266286	8000.126408	12.584205	-0.056934	4.816143
279.320926	8000.049412	12.589210	-0.056944	4.816121
279.091923	7999.992925	12.594215	-0.056902	4.816105
279.291031	7999.987975	12.599219	-0.056939	4.816103
279.299007	8000.016954	12.604224	-0.056940	4.816111
279.430797	8000.031082	12.609229	-0.056965	4.816115
279.309650	8000.072682	12.614234	-0.056942	4.816128
279.374137	8000.101615	12.619239	-0.056954	4.816136
279.166896	7999.995317	12.624243	-0.056915	4.816106
279.176710	8000.000830	12.629248	-0.056917	4.816107
279.117739	7999.898282	12.634253	-0.056906	4.816078
278.936090	8000.107559	12.639258	-0.056872	4.816140
279.101365	7999.895838	12.644263	-0.056903	4.816077
279.106158	8000.048669	12.649267	-0.056904	4.816122
279.231170	8000.090447	12.654272	-0.056927	4.816133
279.260784	7999.888023	12.659277	-0.056932	4.816074
278.990130	8000.010237	12.664282	-0.056882	4.816111
279.179716	7999.926069	12.669287	-0.056917	4.816085
279.429600	7999.927377	12.674291	-0.056964	4.816084
279.228880	7999.971810	12.679296	-0.056926	4.816099
279.159355	7999.912866	12.684301	-0.056913	4.816082
279.358815	8000.054263	12.689306	-0.056950	4.816122
279.470089	8000.121429	12.694311	-0.056971	4.816141
279.243193	8000.024388	12.699315	-0.056929	4.816114
279.201557	8000.058880	12.704320	-0.056921	4.816124
279.310218	7999.921976	12.709325	-0.056941	4.816084
279.035518	8000.129572	12.714330	-0.056890	4.816146
279.271862	7999.920204	12.719335	-0.056934	4.816083
279.282922	7999.981284	12.724339	-0.056936	4.816101
279.154953	8000.048397	12.729344	-0.056912	4.816121
279.216214	7999.973659	12.734349	-0.056923	4.816099
279.413686	7999.912064	12.739354	-0.056960	4.816080
279.470310	8000.031651	12.744359	-0.056970	4.816115
279.221446	7999.908578	12.749363	-0.056924	4.816080
279.251746	7999.974279	12.754368	-0.056930	4.816099
279.532725	7999.841559	12.759373	-0.056982	4.816059
279.209266	8000.042933	12.764378	-0.056922	4.816119
279.577395	7999.996174	12.769383	-0.056990	4.816104
279.503462	7999.991627	12.774387	-0.056976	4.816103
279.317804	8000.096152	12.779392	-0.056942	4.816134
279.431712	7999.972160	12.784397	-0.056963	4.816098
279.416961	7999.997525	12.789402	-0.056960	4.816105
279.355722	7999.899207	12.794407	-0.056948	4.816077
279.182070	7999.949471	12.799411	-0.056916	4.816092
279.242657	7999.984743	12.804416	-0.056927	4.816102
279.328647	7999.880543	12.809421	-0.056943	4.816071
279.156959	7999.878502	12.814426	-0.056911	4.816072
279.230001	7999.873408	12.819431	-0.056925	4.816070
279.410902	7999.927945	12.824435	-0.056958	4.816085
279.454948	8000.130624	12.829440	-0.056967	4.816144
279.560009	7999.892176	12.834445	-0.056986	4.816074
279.419544	7999.906722	12.839450	-0.056960	4.816079
279.572302	8000.000274	12.844455	-0.056988	4.816105
279.246866	8000.025362	12.849459	-0.056928	4.816114
279.184396	8000.024227	12.854464	-0.056916	4.816114
279.354826	7999.971758	12.859469	-0.056948	4.816098
279.450086	8000.063202	12.864474	-0.056965	4.816124
279.412181	8000.064648	12.869479	-0.056958	4.816125
279.259265	7999.991377	12.874483	-0.056930	4.816104
279.319201	8000.085388	12.879488	-0.056941	4.816131
279.320157	8000.002081	12.884493	-0.056941	4.816107
279.255123	8000.074605	12.889498	-0.056929	4.816128
279.184225	8000.003885	12.894503	-0.056915	4.816108
279.285368	7999.979004	12.899507	-0.056934	4.816100
279.245372	8000.061594	12.904512	-0.056927	4.816125
279.338700	7999.956458	12.909517	-0.056944	4.816094
279.200642	8000.054365	12.914522	-0.056918	4.816123
279.369679	7999.973030	12.919527	-0.056950	4.816098
279.472443	8000.024019	12.924531	-0.056969	4.816113
279.204505	8000.185806	12.929536	-0.056919	4.816161
279.308788	8000.034936	12.934541	-0.056938	4.816117
279.288300	8000.030287	12.939546	-0.056934	4.816115
279.396897	7999.874154	12.944551	-0.056954	4.816069
279.384565	8000.017062	12.949555	-0.056952	4.816111
279.129430	8000.158785	12.954560	-0.056905	4.816154
279.434734	7999.880163	12.959565	-0.056961	4.816071
279.211072	7999.959432	12.964570	-0.056920	4.816095
279.273845	7999.939198	12.969575	-0.056931	4.816089
279.230899	7999.973666	12.974579	-0.056923	4.816099
279.267812	8000.043760	12.979584	-0.056930	4.816119
279.252746	7999.874710	12.984589	-0.056927	4.816070
279.194430	7999.989013	12.989594	-0.056916	4.816104
279.351974	7999.890379	12.994599	-0.056945	4.816074
279.355816	8000.022898	12.999603	-0.056946	4.816113
279.207863	8000.125968	13.004608	-0.056919	4.816144
279.355280	7999.964127	13.009613	-0.056946	4.816096
279.244871	8000.223832	13.014618	-0.056926	4.816172
279.309226	7999.968625	13.019623	-0.056937	4.816097
279.375603	8000.153548	13.024627	-0.056950	4.816151
279.288474	8000.049421	13.029632	-0.056933	4.816121
279.453971	7999.954135	13.034637	-0.056964	4.816092
279.435216	7999.970881	13.039642	-0.056961	4.816097
279.486391	8000.000642	13.044647	-0.056970	4.816106
279.466913	7999.887057	13.049651	-0.056966	4.816073
279.370740	8000.106427	13.054656	-0.056948	4.816137
279.458387	7999.947779	13.059661	-0.056965	4.816090
279.294054	8000.134939	13.064666	-0.056934	4.816146
279.324391	8000.003027	13.069671	-0.056940	4.816107
279.330466	7999.946518	13.074675	-0.056941	4.816091
279.346616	7999.968168	13.079680	-0.056944	4.816097
279.420238	7999.976971	13.084685	-0.056957	4.816099
279.344310	8000.003366	13.089690	-0.056943	4.816107
279.527879	7999.961816	13.094695	-0.056977	4.816094
279.674264	8000.064868	13.099699	-0.057004	4.816123
279.575374	8000.199803	13.104704	-0.056986	4.816163
279.659081	8000.021854	13.109709	-0.057001	4.816111
279.388347	8000.061817	13.114714	-0.056951	4.816124
279.248230	7999.909733	13.119719	-0.056925	4.816080
279.439015	7999.999700	13.124723	-0.056960	4.816106
279.326607	8000.141867	13.129728	-0.056939	4.816148
279.339426	8000.037411	13.134733	-0.056942	4.816117
279.367577	8000.005869	13.139738	-0.056947	4.816108
279.341453	7999.957323	13.144743	-0.056942	4.816094
279.399701	7999.919916	13.149747	-0.056953	4.816083
279.133815	8000.191763	13.154752	-0.056903	4.816163
279.197384	7999.981407	13.159757	-0.056915	4.816102
279.282978	8000.117540	13.164762	-0.056931	4.816141
279.323003	7999.994349	13.169767	-0.056938	4.816105
279.598900	7999.876491	13.174771	-0.056989	4.816069
279.618419	8000.125727	13.179776	-0.056993	4.816142
279.580296	7999.875076	13.184781	-0.056986	4.816069
279.424675	8000.058121	13.189786	-0.056957	4.816123
279.529269	7999.998052	13.194791	-0.056976	4.816105
279.411423	8000.002325	13.199795	-0.056954	4.816107
279.380531	7999.938738	13.204800	-0.056949	4.816088
279.456850	7999.812999	13.209805	-0.056963	4.816051
279.440109	8000.010305	13.214810	-0.056960	4.816109
279.271326	8000.076679	13.219815	-0.056928	4.816129
279.446254	8000.086246	13.224819	-0.056961	4.816131
279.323300	8000.195110	13.229824	-0.056938	4.816163
279.323106	8000.006031	13.234829	-0.056938	4.816108
279.450558	8000.084172	13.239834	-0.056961	4.816130
279.543835	8000.068762	13.244839	-0.056979	4.816125
279.676291	8000.027356	13.249843	-0.057003	4.816113
279.410127	8000.041765	13.254848	-0.056954	4.816118
279.698198	7999.926263	13.259853	-0.057007	4.816083
279.471500	7999.892250	13.264858	-0.056965	4.816074
279.353067	7999.959535	13.269863	-0.056943	4.816094
279.347942	7999.981869	13.274867	-0.056942	4.816101
279.507927	8000.121485	13.279872	-0.056972	4.816141
279.369003	7999.875421	13.284877	-0.056945	4.816070
279.266063	8000.044463	13.289882	-0.056926	4.816120
279.280461	7999.937900	13.294887	-0.056929	4.816089
279.285560	7999.980714	13.299891	-0.056930	4.816101
279.307668	8000.111427	13.304896	-0.056934	4.816139
279.373756	7999.944912	13.309901	-0.056946	4.816090
279.440994	8000.078577	13.314906	-0.056959	4.816129
279.586024	8000.142082	13.319911	-0.056986	4.816147
279.589506	7999.995797	13.324915	-0.056986	4.816104
279.721815	8000.018480	13.329920	-0.057011	4.816110
279.785385	7999.882895	13.334925	-0.057022	4.816070
279.667778	7999.871150	13.339930	-0.057000	4.816067
279.425120	7999.913757	13.344935	-0.056955	4.816081
279.544919	7999.873191	13.349939	-0.056977	4.816068
279.367408	8000.037681	13.354944	-0.056944	4.816117
279.421697	7999.911543	13.359949	-0.056954	4.816080
279.557884	8000.001591	13.364954	-0.056980	4.816106
279.625674	7999.894925	13.369959	-0.056992	4.816074
279.430866	7999.919170	13.374963	-0.056956	4.816082
279.518039	7999.970945	13.379968	-0.056972	4.816097
279.508303	7999.851127	13.384973	-0.056970	4.816062
279.319071	8000.003655	13.389978	-0.056935	4.816108
279.353278	7999.941246	13.394983	-0.056941	4.816089
279.489794	7999.847572	13.399987	-0.056967	4.816061
279.632370	7999.983668	13.404992	-0.056993	4.816100
279.659716	7999.890156	13.409997	-0.056998	4.816073
279.521726	8000.043611	13.415002	-0.056973	4.816118
279.499011	7999.949194	13.420007	-0.056968	4.816091
279.493904	7999.966188	13.425011	-0.056967	4.816096
279.582256	8000.017985	13.430016	-0.056984	4.816110
279.688488	7999.819081	13.435021	-0.057003	4.816052
279.476077	8000.104714	13.440026	-0.056964	4.816136
279.547040	7999.810104	13.445031	-0.056977	4.816050
279.725127	7999.905182	13.450035	-0.057010	4.816077
279.625136	7999.980278	13.455040	-0.056991	4.816099
279.520736	7999.855544	13.460045	-0.056972	4.816063
279.418415	8000.184827	13.465050	-0.056953	4.816160
279.474944	7999.875001	13.470055	-0.056963	4.816069
279.523016	7999.982683	13.475059	-0.056972	4.816100
279.309995	8000.090986	13.480064	-0.056932	4.816133
279.536088	7999.920954	13.485069	-0.056974	4.816082
279.500709	7999.904286	13.490074	-0.056968	4.816078
279.473560	7999.991381	13.495079	-0.056963	4.816103
279.664437	7999.882668	13.500083	-0.056998	4.816070
279.524175	8000.123673	13.505088	-0.056972	4.816142
279.460118	7999.932372	13.510093	-0.056960	4.816086
279.454289	8000.005966	13.515098	-0.056959	4.816108
279.488915	8000.010859	13.520103	-0.056965	4.816109
279.527006	7999.953861	13.525107	-0.056972	4.816092
279.721956	7999.991562	13.530112	-0.057009	4.816102
279.616924	7999.994999	13.535117	-0.056989	4.816104
279.506915	8000.050686	13.540122	-0.056968	4.816120
279.393597	7999.988813	13.545127	-0.056947	4.816103
279.537040	7999.974311	13.550131	-0.056974	4.816098
279.547105	8000.087716	13.555136	-0.056976	4.816131
279.684059	7999.891503	13.560141	-0.057001	4.816073
279.554515	8000.131635	13.565146	-0.056977	4.816144
279.457487	7999.936532	13.570151	-0.056959	4.816087
279.447668	7999.944895	13.575155	-0.056957	4.816090
279.450638	8000.027194	13.580160	-0.056957	4.816114
279.692180	8000.001647	13.585165	-0.057002	4.816105
279.670827	7999.892300	13.590170	-0.056998	4.816073
279.694028	7999.875623	13.595175	-0.057003	4.816068
279.729104	8000.014048	13.600179	-0.057009	4.816109
279.555769	7999.883795	13.605184	-0.056977	4.816071
279.535274	7999.993442	13.610189	-0.056973	4.816104
279.534856	8000.047906	13.615194	-0.056973	4.816119
279.542246	8000.117467	13.620199	-0.056974	4.816140
279.707817	8000.068115	13.625203	-0.057005	4.816124
279.649053	8000.176003	13.630208	-0.056994	4.816156
279.635730	7999.898026	13.635213	-0.056991	4.816075
279.621025	8000.127416	13.640218	-0.056989	4.816142
279.605649	8000.039541	13.645223	-0.056986	4.816117
279.803521	7999.968340	13.650227	-0.057022	4.816095
279.584107	7999.986799	13.655232	-0.056981	4.816101
279.723434	7999.935903	13.660237	-0.057007	4.816086
279.507908	8000.011047	13.665242	-0.056967	4.816109
279.556867	8000.030086	13.670247	-0.056976	4.816114
279.730845	7999.989431	13.675251	-0.057009	4.816101
279.507486	7999.989659	13.680256	-0.056967	4.816103
279.784494	7999.891049	13.685261	-0.057018	4.816072
279.717204	7999.904781	13.690266	-0.057006	4.816077
279.660745	8000.124871	13.695271	-0.056995	4.816141
279.655761	7999.904728	13.700275	-0.056994	4.816077
279.472147	8000.009289	13.705280	-0.056960	4.816109
279.579637	7999.989864	13.710285	-0.056980	4.816102
279.562300	7999.998090	13.715290	-0.056977	4.816105
279.642647	8000.016629	13.720295	-0.056992	4.816110
279.513487	7999.802788	13.725299	-0.056967	4.816048
279.611031	8000.072661	13.730304	-0.056986	4.816126
279.775469	7999.958128	13.735309	-0.057016	4.816092
279.487969	7999.915537	13.740314	-0.056963	4.816081
279.554638	7999.957328	13.745319	-0.056975	4.816093
279.561761	7999.960656	13.750323	-0.056976	4.816094
279.548050	7999.988176	13.755328	-0.056974	4.816102
279.583294	7999.861694	13.760333	-0.056980	4.816065
279.513118	8000.018511	13.765338	-0.056967	4.816111
279.649934	7999.981457	13.770343	-0.056992	4.816099
279.800469	7999.886968	13.775347	-0.057020	4.816071
279.384539	8000.003352	13.780352	-0.056943	4.816107
279.760559	7999.909736	13.785357	-0.057013	4.816078
279.657934	7999.951670	13.790362	-0.056994	4.816091
279.783964	7999.889853	13.795367	-0.057017	4.816072
279.867652	7999.889224	13.800371	-0.057033	4.816071
279.614296	8000.189073	13.805376	-0.056986	4.816160
279.706415	8000.032640	13.810381	-0.057003	4.816114
279.486852	8000.138688	13.815386	-0.056962	4.816146
279.738996	8000.048173	13.820391	-0.057009	4.816118
279.859697	8000.026850	13.825395	-0.057031	4.816112
279.774439	7999.964416	13.830400	-0.057015	4.816094
279.843353	7999.911179	13.835405	-0.057028	4.816078
279.977631	7999.985171	13.840410	-0.057053	4.816099
279.767446	8000.016615	13.845415	-0.057014	4.816109
279.804174	7999.795090	13.850419	-0.057020	4.816044
279.609662	7999.974228	13.855424	-0.056984	4.816098
279.742900	7999.926427	13.860429	-0.057009	4.816083
279.682238	8000.037485	13.865434	-0.056997	4.816116
279.669549	7999.975295	13.870439	-0.056995	4.816098
279.688188	8000.019422	13.875443	-0.056998	4.816110
279.775196	8000.088287	13.880448	-0.057015	4.816130
279.783640	7999.923932	13.885453	-0.057016	4.816082
279.752408	8000.002408	13.890458	-0.057010	4.816105
279.704743	7999.978040	13.895463	-0.057001	4.816098
279.575774	8000.046204	13.900467	-0.056977	4.816119
279.727129	7999.972025	13.905472	-0.057005	4.816096
279.835704	7999.964370	13.910477	-0.057025	4.816094
279.740238	8000.131413	13.915482	-0.057008	4.816143
279.745689	8000.066346	13.920487	-0.057009	4.816124
279.811586	7999.969258	13.925491	-0.057021	4.816095
279.604398	8000.124667	13.930496	-0.056982	4.816142
279.657328	7999.930140	13.935501	-0.056992	4.816084
279.691007	8000.033290	13.940506	-0.056998	4.816114
279.602359	8000.018863	13.945511	-0.056982	4.816111
279.579697	7999.999220	13.950515	-0.056977	4.816105
279.506434	7999.982936	13.955520	-0.056964	4.816101
279.660385	7999.832964	13.960525	-0.056992	4.816056
279.622799	8000.072621	13.965530	-0.056985	4.816126
279.466990	7999.987547	13.970535	-0.056956	4.816102
279.715703	7999.949312	13.975539	-0.057002	4.816090
279.620461	8000.104608	13.980544	-0.056985	4.816136
279.695179	7999.912611	13.985549	-0.056998	4.816079
279.700674	7999.999229	13.990554	-0.056999	4.816104
279.669865	7999.971961	13.995559	-0.056994	4.816097
279.667123	7999.927043	14.000563	-0.056993	4.816084
279.658346	8000.102062	14.005568	-0.056991	4.816135
279.675816	8000.008371	14.010573	-0.056995	4.816107
279.791431	8000.002979	14.015578	-0.057016	4.816105
279.876026	8000.042959	14.020583	-0.057032	4.816116
279.781259	7999.980353	14.025587	-0.057014	4.816099
279.616110	8000.146135	14.030592	-0.056983	4.816148
279.665584	7999.890659	14.035597	-0.056992	4.816073
279.881810	8000.002451	14.040602	-0.057033	4.816104
279.892463	8000.120140	14.045607	-0.057035	4.816139
279.843790	7999.904547	14.050611	-0.057025	4.816076
279.892114	7999.970575	14.055616	-0.057034	4.816095
279.817323	7999.881625	14.060621	-0.057020	4.816069
279.613055	8000.048837	14.065626	-0.056982	4.816119
279.628318	7999.942288	14.070631	-0.056985	4.816088
279.858726	7999.856721	14.075635	-0.057028	4.816062
279.658675	7999.964190	14.080640	-0.056991	4.816094
279.806220	7999.990353	14.085645	-0.057018	4.816101
279.683618	7999.991335	14.090650	-0.056995	4.816102
279.797605	8000.084188	14.095655	-0.057016	4.816129
279.621980	8000.054302	14.100659	-0.056984	4.816121
279.516521	8000.000048	14.105664	-0.056964	4.816106
279.764968	7999.895580	14.110669	-0.057010	4.816074
279.823886	7999.988504	14.115674	-0.057021	4.816101
279.719374	7999.993018	14.120679	-0.057002	4.816103
279.835460	7999.897906	14.125683	-0.057023	4.816074
279.469480	8000.099580	14.130688	-0.056955	4.816135
279.655605	7999.904257	14.135693	-0.056989	4.816077
279.622183	7999.889761	14.140698	-0.056983	4.816073
279.693223	8000.044860	14.145703	-0.056996	4.816118
279.822029	7999.923273	14.150707	-0.057020	4.816082
279.800165	7999.990168	14.155712	-0.057016	4.816101
279.806120	8000.012703	14.160717	-0.057017	4.816108
279.798379	7999.951671	14.165722	-0.057016	4.816090
279.778490	7999.985488	14.170727	-0.057012	4.816100
279.858174	7999.998673	14.175731	-0.057027	4.816104
279.815138	7999.894275	14.180736	-0.057019	4.816073
279.778685	8000.019657	14.185741	-0.057012	4.816110
279.827346	8000.161534	14.190746	-0.057021	4.816151
279.785612	8000.044340	14.195751	-0.057013	4.816117
279.892750	7999.975771	14.200755	-0.057033	4.816097
279.752256	8000.103545	14.205760	-0.057007	4.816135
280.034649	7999.866166	14.210765	-0.057059	4.816064
279.764780	7999.995873	14.215770	-0.057009	4.816103
279.663053	8000.192713	14.220775	-0.056990	4.816161
279.954047	8000.065514	14.225779	-0.057044	4.816123
279.803890	8000.184568	14.230784	-0.057016	4.816158
279.836255	7999.952280	14.235789	-0.057022	4.816090
279.824475	7999.952062	14.240794	-0.057020	4.816090
279.727130	7999.915046	14.245799	-0.057002	4.816080
279.796634	7999.618275	14.250803	-0.057014	4.815993

279.619708	7996.277397	14.255808	-0.056979	4.815017
279.827541	7990.755405	14.260813	-0.057014	4.813401
279.702376	7983.988172	14.265818	-0.056986	4.811423
279.583387	7976.654267	14.270823	-0.056959	4.809277
279.655713	7969.068982	14.275827	-0.056968	4.807056
279.610516	7961.213424	14.280832	-0.056954	4.804756
279.744788	7953.399845	14.285837	-0.056974	4.802465
279.627346	7945.436685	14.290842	-0.056947	4.800131
279.587260	7937.460641	14.295847	-0.056934	4.797792
279.406385	7929.439411	14.300851	-0.056895	4.795439
279.273006	7921.381505	14.305856	-0.056865	4.793074
279.377215	7913.391994	14.310861	-0.056879	4.790726
279.386694	7905.386821	14.315866	-0.056876	4.788374
279.262540	7897.380320	14.320871	-0.056847	4.786020
279.252022	7889.422002	14.325875	-0.056840	4.783679
279.239274	7881.404992	14.330880	-0.056833	4.781319
279.126291	7873.432847	14.335885	-0.056806	4.778972
278.937167	7865.395744	14.340890	-0.056766	4.776605
278.879055	7857.367796	14.345895	-0.056750	4.774239
279.084518	7849.401630	14.350899	-0.056783	4.771888
278.908624	7841.327062	14.355904	-0.056745	4.769507
278.753792	7833.402803	14.360909	-0.056710	4.767168
278.732524	7825.379727	14.365914	-0.056701	4.764798
278.705810	7817.408116	14.370919	-0.056691	4.762443
278.923747	7809.411027	14.375923	-0.056726	4.760078
278.759003	7801.376897	14.380928	-0.056690	4.757702
278.662996	7793.389935	14.385933	-0.056667	4.755338
278.596493	7785.349391	14.390938	-0.056650	4.752958
278.729336	7777.255376	14.395943	-0.056669	4.750560
278.743285	7769.350318	14.400947	-0.056666	4.748216
278.521948	7761.347343	14.405952	-0.056620	4.745844
278.483643	7753.371711	14.410957	-0.056607	4.743478
278.341254	7745.365200	14.415962	-0.056576	4.741102
278.391560	7737.327182	14.420967	-0.056580	4.738714
278.413967	7729.355908	14.425971	-0.056579	4.736346
278.361801	7721.313239	14.430976	-0.056564	4.733955
278.340807	7713.324327	14.435981	-0.056555	4.731579
277.944719	7705.323825	14.440986	-0.056475	4.729199
278.104452	7697.264265	14.445991	-0.056500	4.726799
278.323753	7689.341391	14.450995	-0.056536	4.724438
278.013225	7681.364580	14.456000	-0.056472	4.722062
278.155869	7673.314851	14.461005	-0.056494	4.719661
278.027635	7665.403536	14.466010	-0.056465	4.717301
277.950158	7657.316880	14.471015	-0.056445	4.714887
277.860023	7649.306395	14.476019	-0.056423	4.712495
277.678123	7641.293943	14.481024	-0.056384	4.710102
277.816833	7633.274997	14.486029	-0.056404	4.707704
277.858812	7625.295750	14.491034	-0.056407	4.705317
277.820537	7617.318800	14.496039	-0.056394	4.702930
277.940494	7609.358743	14.501043	-0.056412	4.700546
277.588907	7601.323732	14.506048	-0.056341	4.698140
277.576141	7593.304075	14.511053	-0.056333	4.695737
277.451289	7585.332402	14.516058	-0.056305	4.693346
277.302593	7577.211738	14.521063	-0.056272	4.690910
277.354396	7569.292350	14.526067	-0.056276	4.688533
277.406818	7561.270971	14.531072	-0.056280	4.686124
277.480200	7553.301636	14.536077	-0.056289	4.683729
277.398798	7545.318666	14.541082	-0.056268	4.681329
277.259314	7537.290668	14.546087	-0.056237	4.678914
277.302378	7529.353120	14.551091	-0.056240	4.676525
277.042780	7521.241472	14.556096	-0.056186	4.674083
277.103137	7513.191064	14.561101	-0.056192	4.671658
277.318118	7505.222375	14.566106	-0.056227	4.669255
277.219390	7497.189655	14.571111	-0.056203	4.666833
276.938595	7489.235642	14.576115	-0.056146	4.664433
276.979802	7481.319633	14.581120	-0.056148	4.662044
276.836689	7473.243449	14.586125	-0.056116	4.659604
276.880256	7465.281970	14.591130	-0.056119	4.657198
276.650517	7457.216957	14.596135	-0.056071	4.654760
276.772803	7449.272417	14.601139	-0.056089	4.652356
276.561874	7441.177854	14.606144	-0.056044	4.649906
276.810222	7433.219453	14.611149	-0.056085	4.647496
276.696354	7425.200792	14.616154	-0.056059	4.645066
276.495650	7417.261202	14.621159	-0.056016	4.642660
276.571442	7409.209520	14.626163	-0.056025	4.640217
276.519912	7401.269604	14.631168	-0.056010	4.637808
276.618733	7393.247988	14.636173	-0.056023	4.635372
276.278510	7385.222020	14.641178	-0.055954	4.632934
276.374667	7377.167786	14.646183	-0.055967	4.630486
276.364177	7369.224232	14.651187	-0.055960	4.628070
276.139121	7361.161216	14.656192	-0.055913	4.625617
276.073344	7353.212634	14.661197	-0.055895	4.623197
276.092739	7345.233588	14.666202	-0.055893	4.620766
276.254681	7337.208830	14.671207	-0.055918	4.618321
276.060476	7329.216322	14.676211	-0.055877	4.615884
275.821391	7321.142118	14.681216	-0.055827	4.613420
275.987024	7313.171017	14.686221	-0.055853	4.610987
275.705538	7305.197437	14.691226	-0.055795	4.608552
275.766705	7297.154964	14.696231	-0.055801	4.606094
276.028147	7289.205729	14.701235	-0.055845	4.603664
275.784939	7281.209314	14.706240	-0.055794	4.601218
275.782538	7273.200000	14.711245	-0.055788	4.598766
275.719652	7265.173555	14.716250	-0.055771	4.596308
275.612109	7257.121897	14.721255	-0.055746	4.593841
275.452503	7249.146915	14.726259	-0.055711	4.591396
275.517761	7241.155800	14.731264	-0.055718	4.588945
275.526619	7233.133377	14.736269	-0.055714	4.586483
275.401009	7225.145875	14.741274	-0.055686	4.584031
275.363366	7217.138232	14.746279	-0.055673	4.581571
275.283221	7209.177611	14.751283	-0.055653	4.579124
275.296528	7201.149099	14.756288	-0.055650	4.576654
275.215401	7193.147391	14.761293	-0.055630	4.574192
275.269367	7185.126470	14.766298	-0.055635	4.571722
275.357695	7177.115881	14.771303	-0.055646	4.569255
275.261656	7169.160632	14.776307	-0.055623	4.566803
275.107321	7161.116729	14.781312	-0.055589	4.564322
275.018124	7153.197473	14.786317	-0.055567	4.561879
274.917620	7145.148072	14.791322	-0.055543	4.559393
274.907433	7137.177611	14.796327	-0.055536	4.556931
274.942493	7129.146693	14.801331	-0.055537	4.554449
274.812745	7121.121714	14.806336	-0.055508	4.551968
274.729292	7113.080829	14.811341	-0.055487	4.549480
274.528384	7105.139601	14.816346	-0.055444	4.547021
274.818944	7097.112131	14.821351	-0.055493	4.544535
274.641027	7089.218802	14.826355	-0.055455	4.542089
274.460166	7081.126487	14.831360	-0.055416	4.539579
274.654489	7073.176857	14.836365	-0.055447	4.537113
274.461385	7065.101602	14.841370	-0.055405	4.534606
274.341235	7057.088822	14.846375	-0.055378	4.532117
274.404291	7049.105672	14.851379	-0.055384	4.529637
274.285368	7041.153948	14.856384	-0.055357	4.527164
274.249192	7033.108851	14.861389	-0.055345	4.524661
274.343322	7025.169757	14.866394	-0.055357	4.522190
274.360435	7017.124192	14.871399	-0.055355	4.519684
274.352694	7009.158361	14.876403	-0.055348	4.517202
274.234487	7001.099516	14.881408	-0.055321	4.514689
274.158451	6993.057945	14.886413	-0.055301	4.512180
274.249951	6985.061759	14.891418	-0.055313	4.509685
273.912681	6977.067932	14.896423	-0.055245	4.507187
274.118036	6969.057849	14.901427	-0.055278	4.504685
274.094501	6961.098735	14.906432	-0.055268	4.502196
273.918376	6953.060376	14.911437	-0.055230	4.499681
273.825507	6945.119680	14.916442	-0.055208	4.497195
273.873506	6937.074681	14.921447	-0.055211	4.494676
273.736136	6929.071534	14.926451	-0.055181	4.492168
273.514581	6921.048730	14.931456	-0.055134	4.489652
273.629030	6913.090354	14.936461	-0.055150	4.487155
273.594878	6905.058110	14.941466	-0.055138	4.484634
273.380203	6897.105542	14.946471	-0.055093	4.482136
273.514362	6889.069922	14.951475	-0.055113	4.479611
273.400409	6881.082772	14.956480	-0.055086	4.477099
273.672056	6873.054851	14.961485	-0.055132	4.474575
273.304438	6865.041485	14.966490	-0.055058	4.472051
273.289741	6857.027346	14.971495	-0.055050	4.469527
273.430899	6849.057785	14.976499	-0.055071	4.467016
273.315070	6841.023023	14.981504	-0.055044	4.464482
273.352055	6833.078343	14.986509	-0.055046	4.461976
273.304621	6825.046076	14.991514	-0.055032	4.459440
273.047652	6817.036479	14.996519	-0.054979	4.456909
273.019157	6809.049768	15.001523	-0.054968	4.454385
273.023493	6800.994196	15.006528	-0.054964	4.451838
273.118261	6793.015210	15.011533	-0.054976	4.449314
272.861277	6785.054656	15.016538	-0.054923	4.446793
272.943382	6776.988315	15.021543	-0.054933	4.444238
272.877309	6769.064263	15.026547	-0.054915	4.441726
272.698793	6761.027989	15.031552	-0.054877	4.439177
272.612313	6753.043471	15.036557	-0.054855	4.436643
272.800793	6744.989322	15.041562	-0.054885	4.434087
272.660407	6736.949841	15.046567	-0.054854	4.431533
272.705109	6729.038352	15.051571	-0.054857	4.429018
272.639228	6720.962038	15.056576	-0.054839	4.426449
272.751431	6712.994000	15.061581	-0.054855	4.423914
272.384890	6705.017368	15.066586	-0.054781	4.421373
272.423414	6696.999747	15.071591	-0.054783	4.418819
272.375719	6689.027120	15.076595	-0.054769	4.416277
272.184603	6680.982852	15.081600	-0.054728	4.413711
272.123683	6672.978646	15.086605	-0.054712	4.411156
272.245242	6665.017513	15.091610	-0.054729	4.408614
272.097829	6656.964272	15.096615	-0.054696	4.406041
272.172408	6649.019885	15.101619	-0.054705	4.403501
272.039488	6641.040261	15.106624	-0.054675	4.400948
272.140978	6633.026639	15.111629	-0.054689	4.398384
271.944168	6625.052491	15.116634	-0.054647	4.395829
271.982346	6616.983928	15.121639	-0.054649	4.393244
272.085507	6609.009604	15.126643	-0.054662	4.390687
271.918658	6600.978077	15.131648	-0.054626	4.388110
271.862393	6592.968991	15.136653	-0.054610	4.385538
271.861005	6585.022032	15.141658	-0.054605	4.382986
271.732139	6576.976952	15.146663	-0.054576	4.380400
271.583446	6569.065131	15.151667	-0.054543	4.377855
271.607403	6561.025056	15.156672	-0.054542	4.375268
271.664009	6552.991111	15.161677	-0.054547	4.372681
271.627218	6544.986785	15.166682	-0.054535	4.370103
271.438545	6537.000537	15.171687	-0.054495	4.367527
271.546191	6529.002187	15.176691	-0.054509	4.364948
271.186753	6521.024687	15.181696	-0.054437	4.362372
271.201354	6513.000775	15.186701	-0.054435	4.359781
271.356188	6505.053431	15.191706	-0.054458	4.357214
271.233268	6496.978802	15.196711	-0.054430	4.354602
271.259550	6488.895655	15.201715	-0.054430	4.351988
271.225999	6480.901423	15.206720	-0.054418	4.349400
271.106501	6472.956987	15.211725	-0.054391	4.346826
270.997619	6464.958357	15.216730	-0.054365	4.344233
270.850018	6456.973976	15.221735	-0.054332	4.341643
270.984111	6448.957110	15.226739	-0.054352	4.339043
270.926692	6440.993052	15.231744	-0.054336	4.336457
270.854017	6432.941850	15.236749	-0.054317	4.333841
270.934713	6424.971158	15.241754	-0.054327	4.331251
270.727927	6416.972738	15.246759	-0.054283	4.328648
270.679095	6408.973063	15.251763	-0.054269	4.326044
270.727851	6400.988647	15.256768	-0.054273	4.323445
270.601812	6392.959080	15.261773	-0.054244	4.320827
270.614567	6384.998482	15.266778	-0.054241	4.318232
270.441311	6376.941444	15.271783	-0.054203	4.315602
270.536828	6368.942831	15.276787	-0.054216	4.312992
270.593769	6360.887766	15.281792	-0.054221	4.310362
270.508589	6352.981127	15.286797	-0.054200	4.307777
270.439208	6344.931949	15.291802	-0.054182	4.305144
270.430751	6336.938818	15.296807	-0.054175	4.302528
270.259561	6328.979992	15.301811	-0.054138	4.299921
270.195426	6320.951217	15.306816	-0.054121	4.297290
270.278495	6312.923992	15.311821	-0.054131	4.294659
270.407619	6304.904393	15.316826	-0.054150	4.292030
270.164372	6296.896514	15.321831	-0.054099	4.289399
270.069679	6288.975659	15.326835	-0.054076	4.286797
269.924957	6280.917449	15.331840	-0.054044	4.284148
269.821225	6272.974350	15.336845	-0.054020	4.281535
269.893544	6264.956941	15.341850	-0.054028	4.278898
269.739944	6256.942400	15.346855	-0.053994	4.276258
269.948249	6248.935318	15.351859	-0.054027	4.273621
269.783306	6240.853385	15.356864	-0.053991	4.270956
269.825871	6232.923708	15.361869	-0.053994	4.268341
269.765893	6224.882325	15.366874	-0.053978	4.265686
269.584957	6216.916156	15.371879	-0.053939	4.263054
269.692893	6208.924913	15.376883	-0.053953	4.260414
269.665085	6200.951533	15.381888	-0.053943	4.257777
269.517822	6192.907934	15.386893	-0.053910	4.255114
269.301912	6184.911773	15.391898	-0.053865	4.252465
269.371798	6176.885817	15.396903	-0.053873	4.249806
269.384580	6168.954882	15.401907	-0.053870	4.247177
269.131097	6160.914627	15.406912	-0.053817	4.244508
268.991936	6152.959198	15.411917	-0.053786	4.241866
269.091150	6144.929947	15.416922	-0.053799	4.239200
269.015045	6136.975317	15.421927	-0.053780	4.236556
269.234345	6128.955597	15.426931	-0.053815	4.233891
269.132866	6120.922561	15.431936	-0.053791	4.231217
269.062614	6112.927523	15.436941	-0.053773	4.228554
269.029854	6104.931817	15.441946	-0.053762	4.225890
268.914324	6096.946332	15.446951	-0.053735	4.223226
269.001938	6088.952650	15.451955	-0.053746	4.220561
268.877232	6080.954206	15.456960	-0.053717	4.217889
268.932872	6072.956598	15.461965	-0.053722	4.215218
268.843055	6064.944941	15.466970	-0.053700	4.212540
268.723600	6056.898236	15.471975	-0.053673	4.209847
268.664836	6048.996693	15.476979	-0.053657	4.207202
268.508113	6040.916669	15.481984	-0.053622	4.204495
268.422224	6032.987889	15.486989	-0.053601	4.201837
268.407148	6024.969886	15.491994	-0.053593	4.199149
268.442828	6016.971307	15.496999	-0.053594	4.196465
268.438142	6008.918646	15.502003	-0.053588	4.193762
268.383101	6000.814209	15.507008	-0.053573	4.191038
268.234125	5992.886012	15.512013	-0.053540	4.188371
268.271707	5984.868060	15.517018	-0.053541	4.185675
268.025995	5976.920698	15.522023	-0.053490	4.182997
268.198150	5968.912551	15.527027	-0.053517	4.180301
268.281121	5960.942892	15.532032	-0.053527	4.177616
268.261682	5952.928850	15.537037	-0.053518	4.174913
268.194453	5944.938194	15.542042	-0.053501	4.172216
268.016869	5936.867581	15.547047	-0.053462	4.169488
267.938164	5928.952434	15.552051	-0.053442	4.166813
267.648699	5920.908081	15.557056	-0.053383	4.164089
267.574228	5912.935840	15.562061	-0.053364	4.161391
267.793390	5904.948037	15.567066	-0.053400	4.158689
267.510155	5896.927705	15.572071	-0.053342	4.155968
267.839744	5888.917100	15.577075	-0.053398	4.153256
267.744590	5880.866096	15.582080	-0.053375	4.150524
267.518394	5872.881878	15.587085	-0.053327	4.147811
267.396236	5864.918736	15.592090	-0.053299	4.145105
267.292295	5856.938193	15.597095	-0.053275	4.142391
267.572576	5848.898318	15.602099	-0.053322	4.139659
267.222892	5840.925803	15.607104	-0.053251	4.136941
267.314394	5832.899330	15.612109	-0.053263	4.134209
267.296494	5824.902111	15.617114	-0.053254	4.131483
267.241802	5816.847423	15.622119	-0.053239	4.128735
267.211319	5808.882319	15.627123	-0.053228	4.126017
267.285812	5800.894986	15.632128	-0.053237	4.123290
267.057053	5792.931990	15.637133	-0.053189	4.120566
266.843736	5784.965592	15.642138	-0.053144	4.117839
266.733510	5776.916924	15.647143	-0.053118	4.115084
266.965308	5768.866723	15.652147	-0.053156	4.112330
267.067752	5760.850241	15.657152	-0.053170	4.109585
266.766720	5752.892151	15.662157	-0.053108	4.106852
266.650033	5744.878095	15.667162	-0.053081	4.104101
266.632710	5736.903046	15.672167	-0.053073	4.101363
266.749022	5728.973765	15.677171	-0.053089	4.098640
266.566995	5720.937456	15.682176	-0.053050	4.095875
266.522270	5712.909638	15.687181	-0.053036	4.093113
266.666106	5704.900961	15.692186	-0.053058	4.090357
266.503008	5696.905712	15.697191	-0.053022	4.087601
266.535689	5688.895751	15.702195	-0.053023	4.084840
266.534608	5680.988402	15.707200	-0.053018	4.082113
266.228330	5672.949890	15.712205	-0.052955	4.079334
266.293578	5665.006431	15.717210	-0.052962	4.076591
266.189121	5656.941310	15.722215	-0.052938	4.073801
266.282704	5648.926309	15.727219	-0.052950	4.071030
266.106224	5640.944537	15.732224	-0.052912	4.068265
266.266365	5632.910755	15.737229	-0.052936	4.065485
266.105088	5624.978975	15.742234	-0.052901	4.062733
265.964864	5616.930323	15.747239	-0.052869	4.059940
265.997895	5608.992696	15.752243	-0.052870	4.057185
265.976695	5600.935050	15.757248	-0.052861	4.054386
265.968515	5592.922864	15.762253	-0.052854	4.051601
265.859556	5584.953518	15.767258	-0.052829	4.048828
265.751425	5576.934951	15.772263	-0.052803	4.046036
265.742210	5568.978826	15.777267	-0.052796	4.043265
265.563775	5560.949216	15.782272	-0.052758	4.040464
265.713585	5552.977802	15.787277	-0.052780	4.037686
265.587711	5544.975962	15.792282	-0.052752	4.034891
265.356030	5536.844773	15.797287	-0.052703	4.032048
265.534393	5528.896771	15.802291	-0.052731	4.029273
265.479959	5520.903376	15.807296	-0.052716	4.026477
265.483443	5512.904178	15.812301	-0.052711	4.023677
265.312251	5504.960809	15.817306	-0.052674	4.020893
265.396175	5496.921213	15.822311	-0.052684	4.018076
265.132440	5488.951196	15.827315	-0.052630	4.015277
265.004208	5480.919613	15.832320	-0.052601	4.012456
265.248296	5472.890831	15.837325	-0.052641	4.009640
265.136620	5464.934684	15.842330	-0.052615	4.006842
265.049907	5456.896974	15.847335	-0.052594	4.004014
265.013402	5448.983366	15.852339	-0.052582	4.001228
265.125675	5440.942857	15.857344	-0.052597	3.998398
264.984628	5432.942319	15.862349	-0.052566	3.995576
264.974236	5424.925721	15.867354	-0.052558	3.992749
264.824765	5416.876858	15.872359	-0.052525	3.989905
264.841498	5408.932327	15.877363	-0.052523	3.987100
264.808055	5400.922377	15.882368	-0.052512	3.984268
264.797852	5392.978849	15.887373	-0.052505	3.981458
264.572290	5385.000536	15.892378	-0.052457	3.978631
264.444698	5376.943316	15.897383	-0.052428	3.975775
264.604650	5368.941190	15.902387	-0.052453	3.972941
264.615875	5360.908494	15.907392	-0.052450	3.970092
264.458771	5352.944790	15.912397	-0.052415	3.967262
264.389238	5344.983627	15.917402	-0.052397	3.964433
264.362182	5337.005120	15.922407	-0.052387	3.961596
264.322158	5329.004006	15.927411	-0.052374	3.958749
264.188531	5321.016609	15.932416	-0.052344	3.955904
264.282298	5312.956763	15.937421	-0.052356	3.953034
264.458687	5304.936438	15.942426	-0.052383	3.950178
264.164676	5296.978496	15.947431	-0.052323	3.947333
264.176761	5288.969741	15.952435	-0.052320	3.944474
264.194547	5281.016309	15.957440	-0.052319	3.941633
264.037321	5273.027343	15.962445	-0.052284	3.938774
263.974626	5265.044012	15.967450	-0.052267	3.935916
263.970529	5256.965159	15.972455	-0.052261	3.933023
263.929529	5248.995970	15.977459	-0.052248	3.930167
263.694516	5241.008216	15.982464	-0.052199	3.927299
263.648877	5232.979643	15.987469	-0.052185	3.924417
263.676280	5225.025495	15.992474	-0.052185	3.921561
263.630667	5217.004360	15.997479	-0.052171	3.918677
263.460424	5209.037044	16.002483	-0.052134	3.915809
263.393764	5201.003675	16.007488	-0.052117	3.912916
263.372894	5192.979170	16.012493	-0.052108	3.910026
263.369714	5185.042839	16.017498	-0.052102	3.907165
263.312881	5176.993930	16.022503	-0.052086	3.904260
263.336198	5169.039458	16.027507	-0.052085	3.901389
263.153850	5161.020166	16.032512	-0.052046	3.898489
263.223160	5153.016432	16.037517	-0.052053	3.895597
263.243348	5145.005627	16.042522	-0.052052	3.892699
262.895952	5136.970699	16.047527	-0.051982	3.889783
262.878869	5129.069475	16.052531	-0.051973	3.886920
263.091376	5120.991687	16.057536	-0.052008	3.883995
262.850458	5113.029661	16.062541	-0.051958	3.881101
262.817735	5105.053281	16.067546	-0.051946	3.878204
262.921145	5097.007856	16.072551	-0.051960	3.875282
262.874182	5088.810818	16.077555	-0.051946	3.872300
262.797794	5080.824897	16.082560	-0.051927	3.869392
262.666495	5072.928488	16.087565	-0.051897	3.866513
262.811590	5065.001813	16.092570	-0.051919	3.863627
262.466758	5056.937957	16.097575	-0.051849	3.860678
262.622525	5049.001295	16.102579	-0.051873	3.857784
262.588137	5040.976613	16.107584	-0.051861	3.854851
262.502743	5032.981316	16.112589	-0.051840	3.851926
262.667450	5024.982760	16.117594	-0.051866	3.849003
262.434402	5017.002614	16.122599	-0.051817	3.846076
262.659042	5009.021392	16.127603	-0.051853	3.843156
262.402006	5001.060786	16.132608	-0.051800	3.840231
262.169212	4993.082913	16.137613	-0.051752	3.837298
262.255386	4985.081645	16.142618	-0.051763	3.834361
262.013039	4977.048746	16.147623	-0.051712	3.831403
262.004847	4969.039611	16.152627	-0.051705	3.828457
262.041154	4961.071453	16.157632	-0.051707	3.825524
262.084780	4953.063246	16.162637	-0.051710	3.822574
261.968353	4945.087177	16.167642	-0.051683	3.819631
261.823826	4937.092690	16.172647	-0.051651	3.816678
261.905469	4929.113566	16.177651	-0.051661	3.813733
261.852209	4921.076502	16.182656	-0.051645	3.810761
261.753830	4913.078696	16.187661	-0.051622	3.807801
261.914528	4905.102622	16.192666	-0.051646	3.804852
261.546869	4897.138704	16.197671	-0.051573	3.801894
261.592675	4889.151336	16.202675	-0.051576	3.798933
261.735772	4881.136777	16.207680	-0.051597	3.795963
261.698186	4873.075086	16.212685	-0.051585	3.792969
261.434744	4865.103526	16.217690	-0.051531	3.790000
261.284085	4857.079694	16.222695	-0.051497	3.787013
261.262686	4849.116706	16.227699	-0.051488	3.784049
261.075999	4841.116950	16.232704	-0.051448	3.781065
261.009742	4833.103071	16.237709	-0.051431	3.778076
261.329389	4825.103588	16.242714	-0.051485	3.775098
261.078372	4817.115050	16.247719	-0.051433	3.772110
260.839747	4809.126373	16.252723	-0.051383	3.769119
260.862935	4801.104237	16.257728	-0.051382	3.766120
260.878224	4793.115646	16.262733	-0.051380	3.763130
260.736547	4785.145383	16.267738	-0.051348	3.760141
260.728479	4777.153450	16.272743	-0.051341	3.757145
261.069736	4769.132529	16.277747	-0.051400	3.754144
261.019231	4761.101874	16.282752	-0.051385	3.751127
260.659485	4753.099947	16.287757	-0.051313	3.748112
260.936182	4745.103736	16.292762	-0.051359	3.745111
260.663615	4737.156755	16.297767	-0.051303	3.742114
260.598031	4729.167861	16.302771	-0.051285	3.739103
260.439828	4721.196141	16.307776	-0.051251	3.736094
260.452070	4713.164909	16.312781	-0.051248	3.733064
260.398896	4705.126095	16.317786	-0.051232	3.730027
260.044708	4697.190307	16.322791	-0.051161	3.727020
260.185675	4689.178040	16.327795	-0.051182	3.723993
260.121214	4681.197527	16.332800	-0.051165	3.720970
260.079554	4673.214680	16.337805	-0.051152	3.717945
260.322392	4665.191533	16.342810	-0.051192	3.714909
260.215403	4657.071234	16.347815	-0.051167	3.711825
260.236311	4649.101609	16.352819	-0.051165	3.708799
260.065500	4641.139243	16.357824	-0.051128	3.705768
259.944600	4633.198322	16.362829	-0.051101	3.702745
259.790332	4625.225106	16.367834	-0.051067	3.699705
259.534395	4617.265073	16.372839	-0.051014	3.696666
259.691824	4609.227683	16.377843	-0.051038	3.693605
259.775915	4601.192656	16.382848	-0.051048	3.690540
259.713321	4593.225289	16.387853	-0.051031	3.687495
259.732614	4585.237967	16.392858	-0.051029	3.684442
259.444207	4577.280670	16.397863	-0.050971	3.681391
259.586209	4569.257022	16.402867	-0.050992	3.678322
259.509006	4561.256892	16.407872	-0.050972	3.675254
259.432404	4553.249612	16.412877	-0.050952	3.672180
259.363204	4545.253463	16.417882	-0.050934	3.669109
259.352168	4537.248811	16.422887	-0.050927	3.666033
259.340979	4529.272810	16.427891	-0.050920	3.662966
259.378749	4521.245902	16.432896	-0.050921	3.659878
259.145285	4513.302271	16.437901	-0.050873	3.656812
259.245714	4505.270112	16.442906	-0.050886	3.653718
259.140090	4497.223832	16.447911	-0.050861	3.650611
258.935250	4489.283288	16.452915	-0.050818	3.647539
258.720490	4481.279958	16.457920	-0.050773	3.644440
258.706817	4473.310200	16.462925	-0.050765	3.641357
258.815054	4465.330024	16.467930	-0.050780	3.638270
258.797597	4457.288665	16.472935	-0.050771	3.635153
258.603413	4449.275188	16.477939	-0.050730	3.632041
258.568649	4441.245650	16.482944	-0.050718	3.628923
258.549836	4433.254868	16.487949	-0.050709	3.625818
258.671920	4425.322999	16.492954	-0.050727	3.622737
258.560210	4417.308996	16.497959	-0.050701	3.619616
258.621890	4409.359607	16.502963	-0.050707	3.616521
258.248339	4401.342492	16.507968	-0.050632	3.613386
258.334232	4393.309169	16.512973	-0.050643	3.610254
258.449640	4385.331059	16.517978	-0.050659	3.607141
258.292553	4377.355004	16.522983	-0.050624	3.604020
258.454733	4369.367404	16.527987	-0.050649	3.600899
258.304126	4361.418349	16.532992	-0.050616	3.597783
258.290873	4353.388470	16.537997	-0.050608	3.594636
258.152225	4345.376144	16.543002	-0.050577	3.591490
258.136201	4337.366933	16.548007	-0.050569	3.588345
258.228523	4329.390367	16.553011	-0.050581	3.585214
258.053608	4321.425612	16.558016	-0.050543	3.582077
257.919106	4313.426163	16.563021	-0.050513	3.578925
257.932569	4305.458016	16.568026	-0.050510	3.575786
257.760609	4297.412127	16.573031	-0.050473	3.572609
257.756246	4289.409568	16.578035	-0.050467	3.569451
257.766607	4281.421720	16.583040	-0.050463	3.566296
257.686461	4273.446747	16.588045	-0.050443	3.563141
257.843265	4265.437906	16.593050	-0.050467	3.559976
257.725341	4257.485404	16.598055	-0.050440	3.556823
257.767520	4249.418823	16.603059	-0.050442	3.553627
257.594113	4241.352556	16.608064	-0.050405	3.550422
257.683520	4233.392909	16.613069	-0.050416	3.547263
257.406659	4225.460371	16.618074	-0.050359	3.544102
257.352243	4217.439299	16.623079	-0.050344	3.540910
257.353604	4209.500497	16.628083	-0.050339	3.537749
257.338737	4201.467430	16.633088	-0.050331	3.534547
257.064096	4193.432149	16.638093	-0.050275	3.531333
257.054273	4185.477455	16.643098	-0.050267	3.528157
256.992394	4177.447954	16.648103	-0.050251	3.524946
256.921346	4169.500609	16.653107	-0.050232	3.521765
256.849839	4161.497381	16.658112	-0.050214	3.518559
256.940550	4153.494641	16.663117	-0.050225	3.515355
257.068897	4145.487744	16.668122	-0.050244	3.512147
256.923580	4137.487193	16.673127	-0.050212	3.508931
256.736316	4129.517446	16.678131	-0.050171	3.505723
256.627124	4121.562298	16.683136	-0.050146	3.502520
256.618029	4113.549433	16.688141	-0.050139	3.499294
256.679589	4105.604358	16.693146	-0.050145	3.496095
256.449345	4097.579178	16.698151	-0.050097	3.492851
256.336729	4089.569472	16.703155	-0.050071	3.489614
256.278762	4081.612444	16.708160	-0.050055	3.486397
256.158423	4073.601285	16.713165	-0.050027	3.483153
256.195470	4065.638572	16.718170	-0.050029	3.479931
256.001445	4057.662001	16.723175	-0.049987	3.476693
255.955266	4049.630593	16.728179	-0.049973	3.473434
256.099130	4041.576450	16.733184	-0.049995	3.470169
255.969947	4033.592025	16.738189	-0.049966	3.466921
256.014096	4025.621417	16.743194	-0.049968	3.463681
255.969386	4017.611626	16.748199	-0.049955	3.460418
255.993711	4009.661374	16.753203	-0.049954	3.457180
255.957035	4001.639257	16.758208	-0.049942	3.453907
255.756459	3993.625599	16.763213	-0.049899	3.450628
255.993354	3985.668703	16.768218	-0.049938	3.447385
255.852539	3977.654077	16.773223	-0.049907	3.444102
255.570740	3969.710312	16.778227	-0.049849	3.440840
255.474762	3961.707480	16.783232	-0.049826	3.437558
255.535058	3953.667025	16.788237	-0.049832	3.434261
255.494310	3945.670557	16.793242	-0.049819	3.430977
255.390911	3937.699757	16.798247	-0.049795	3.427697
255.641642	3929.666901	16.803251	-0.049836	3.424401
255.532652	3921.766453	16.808256	-0.049810	3.421144
255.422758	3913.742681	16.813261	-0.049785	3.417833
255.396025	3905.761534	16.818266	-0.049774	3.414540
255.220383	3897.749696	16.823271	-0.049736	3.411225
255.104641	3889.772511	16.828275	-0.049710	3.407923
255.216782	3881.732296	16.833280	-0.049725	3.404600
255.340224	3873.772030	16.838285	-0.049743	3.401308
255.377230	3865.828836	16.843290	-0.049745	3.398016
255.072464	3857.792364	16.848295	-0.049683	3.394670
255.281109	3849.695701	16.853299	-0.049716	3.391314
255.083120	3841.751193	16.858304	-0.049674	3.388004
254.716618	3833.793398	16.863309	-0.049601	3.384679
254.725027	3825.861617	16.868314	-0.049597	3.381375
254.836266	3817.824948	16.873319	-0.049612	3.378027
254.453474	3809.865445	16.878323	-0.049536	3.374691
254.437476	3801.856165	16.883328	-0.049528	3.371343
254.369012	3793.844370	16.888333	-0.049510	3.367990
254.520164	3785.833900	16.893338	-0.049532	3.364641
254.416051	3777.887274	16.898343	-0.049508	3.361307
254.294950	3769.929208	16.903347	-0.049480	3.357964
254.474941	3761.905132	16.908352	-0.049508	3.354600
254.435541	3753.852861	16.913357	-0.049496	3.351214
254.394755	3745.889700	16.918362	-0.049483	3.347861
254.247156	3737.867417	16.923367	-0.049450	3.344477
254.331141	3729.945129	16.928371	-0.049460	3.341139
253.960510	3721.976816	16.933376	-0.049386	3.337763
254.213762	3713.927316	16.938381	-0.049428	3.334371
254.137834	3705.929931	16.943386	-0.049409	3.330986
253.903576	3697.936051	16.948391	-0.049360	3.327593
254.006670	3689.980694	16.953395	-0.049374	3.324225
253.732195	3682.017772	16.958400	-0.049317	3.320837
253.598796	3674.017703	16.963405	-0.049287	3.317434
253.663741	3666.026133	16.968410	-0.049294	3.314040
253.662737	3657.961995	16.973415	-0.049289	3.310608
253.752001	3649.998627	16.978419	-0.049300	3.307219
253.609871	3642.015514	16.983424	-0.049268	3.303809
253.445685	3634.031700	16.988429	-0.049232	3.300395
253.557780	3626.064595	16.993434	-0.049248	3.296995
253.353110	3618.068154	16.998439	-0.049205	3.293567
253.544593	3610.039032	17.003443	-0.049235	3.290136
253.508458	3602.094565	17.008448	-0.049223	3.286729
253.306224	3594.112855	17.013453	-0.049180	3.283297
253.225928	3586.120673	17.018458	-0.049160	3.279860
253.034543	3578.160677	17.023463	-0.049119	3.276430
253.196551	3570.132352	17.028467	-0.049144	3.272981
253.014488	3562.113771	17.033472	-0.049105	3.269519
252.915511	3554.129539	17.038477	-0.049081	3.266071
252.915287	3546.179527	17.043482	-0.049076	3.262638
252.656294	3538.171877	17.048487	-0.049022	3.259166
252.703175	3530.176780	17.053491	-0.049026	3.255708
252.738668	3522.171749	17.058496	-0.049027	3.252242
252.672239	3514.162248	17.063501	-0.049009	3.248766
252.688419	3506.196197	17.068506	-0.049007	3.245308
252.711709	3498.212132	17.073511	-0.049006	3.241839
252.727447	3490.237299	17.078515	-0.049004	3.238370
252.502095	3482.273885	17.083520	-0.048957	3.234893
252.392284	3474.188957	17.088525	-0.048931	3.231364
252.462412	3466.228520	17.093530	-0.048939	3.227892
252.500157	3458.193925	17.098535	-0.048940	3.224383
252.272707	3450.276175	17.103539	-0.048893	3.220910
252.382537	3442.290057	17.108544	-0.048908	3.217418
252.130363	3434.310049	17.113549	-0.048856	3.213909
252.031213	3426.300394	17.118554	-0.048832	3.210390
251.956737	3418.307205	17.123559	-0.048813	3.206875
252.074813	3410.330274	17.128563	-0.048830	3.203372
251.956500	3402.376470	17.133568	-0.048802	3.199865
251.792083	3394.391197	17.138573	-0.048767	3.196338
251.884410	3386.383486	17.143578	-0.048779	3.192808
251.662067	3378.376248	17.148583	-0.048732	3.189262
251.756586	3370.378298	17.153587	-0.048744	3.185729
251.731776	3362.416735	17.158592	-0.048734	3.182203
251.674810	3354.420613	17.163597	-0.048718	3.178656
251.561402	3346.457823	17.168602	-0.048692	3.175118
251.440717	3338.433021	17.173607	-0.048664	3.171548
251.571271	3330.431817	17.178611	-0.048683	3.167995
251.572886	3322.442805	17.183616	-0.048678	3.164438
251.413078	3314.502818	17.188621	-0.048643	3.160892
251.415231	3306.524735	17.193626	-0.048639	3.157332
251.333197	3298.512804	17.198631	-0.048618	3.153749
251.258404	3290.505133	17.203635	-0.048599	3.150165
251.247443	3282.516452	17.208640	-0.048592	3.146587
251.111122	3274.550446	17.213645	-0.048561	3.143010
251.046275	3266.575492	17.218650	-0.048544	3.139428
251.105846	3258.585028	17.223655	-0.048549	3.135841
251.020959	3250.579661	17.228659	-0.048528	3.132236
250.908444	3242.600812	17.233664	-0.048502	3.128638
250.859253	3234.584152	17.238669	-0.048488	3.125022
250.929002	3226.672241	17.243674	-0.048495	3.121453
250.746973	3218.666433	17.248679	-0.048456	3.117828
250.685888	3210.679463	17.253683	-0.048440	3.114211
250.620507	3202.685008	17.258688	-0.048422	3.110587
250.483071	3194.685722	17.263693	-0.048391	3.106954
250.460511	3186.717439	17.268698	-0.048382	3.103335
250.580999	3178.687932	17.273703	-0.048399	3.099691
250.710222	3170.722475	17.278707	-0.048418	3.096072
250.291211	3162.744371	17.283712	-0.048335	3.092418
250.122689	3154.741932	17.288717	-0.048298	3.088760
250.386299	3146.749419	17.293722	-0.048342	3.085122
250.212559	3138.830651	17.298727	-0.048304	3.081493
250.243355	3130.820267	17.303731	-0.048305	3.077827
250.168711	3122.822567	17.308736	-0.048285	3.074158
250.226453	3114.725873	17.313741	-0.048291	3.070446
250.171071	3106.778765	17.318746	-0.048275	3.066792
250.067078	3098.805394	17.323751	-0.048251	3.063120
250.104199	3090.836771	17.328755	-0.048252	3.059451
250.038612	3082.886126	17.333760	-0.048235	3.055782
249.802683	3074.883380	17.338765	-0.048186	3.052077
249.838839	3066.898420	17.343770	-0.048187	3.048388
249.836478	3058.900088	17.348775	-0.048182	3.044687
249.752182	3050.980508	17.353779	-0.048161	3.041013
249.700309	3043.003981	17.358784	-0.048146	3.037311
249.506981	3034.992675	17.363789	-0.048104	3.033580
249.493329	3026.994240	17.368794	-0.048097	3.029860
249.343399	3018.994273	17.373799	-0.048063	3.026128
249.308303	3011.029831	17.378803	-0.048052	3.022414
249.227615	3003.059882	17.383808	-0.048031	3.018690
249.187495	2995.056199	17.388813	-0.048019	3.014947
249.269867	2987.048373	17.393818	-0.048029	3.011204
249.232393	2979.059651	17.398823	-0.048016	3.007460
249.141950	2971.099745	17.403827	-0.047994	3.003722
249.169783	2963.120126	17.408832	-0.047994	2.999975
249.045312	2955.159160	17.413837	-0.047966	2.996225
248.974702	2947.138945	17.418842	-0.047947	2.992445
248.869500	2939.144462	17.423847	-0.047923	2.988671
248.789217	2931.163451	17.428851	-0.047902	2.984900
248.741723	2923.208245	17.433856	-0.047888	2.981138
248.593587	2915.226967	17.438861	-0.047855	2.977353
248.775247	2907.242621	17.443866	-0.047884	2.973579
248.665112	2899.227683	17.448871	-0.047858	2.969771
248.662142	2891.268803	17.453875	-0.047852	2.965990
248.403533	2883.330972	17.458880	-0.047799	2.962201
248.319389	2875.345467	17.463885	-0.047778	2.958393
248.278224	2867.355869	17.468890	-0.047765	2.954581
248.259516	2859.319963	17.473895	-0.047756	2.950743
248.498849	2851.332677	17.478899	-0.047796	2.946936
248.365559	2843.384006	17.483904	-0.047766	2.943124
248.186734	2835.405712	17.488909	-0.047727	2.939290
248.274876	2827.440904	17.493914	-0.047738	2.935471
248.337205	2819.403523	17.498919	-0.047745	2.931612
248.166113	2811.461671	17.503923	-0.047708	2.927781
248.173222	2803.474674	17.508928	-0.047704	2.923932
248.083302	2795.492594	17.513933	-0.047682	2.920076
248.107801	2787.567384	17.518938	-0.047681	2.916248
247.749637	2779.517699	17.523943	-0.047609	2.912335
247.825983	2771.487476	17.528947	-0.047618	2.908448
247.659118	2763.528069	17.533952	-0.047582	2.904578
247.484421	2755.575724	17.538957	-0.047544	2.900706
247.511587	2747.614436	17.543962	-0.047544	2.896835
247.405192	2739.593951	17.548967	-0.047519	2.892923
247.478620	2731.596491	17.553971	-0.047527	2.889026
247.427003	2723.636398	17.558976	-0.047512	2.885136
247.539074	2715.668923	17.563981	-0.047528	2.881246
247.427556	2707.712133	17.568986	-0.047502	2.877343
247.190776	2699.727963	17.573991	-0.047452	2.873415
247.338581	2691.700542	17.578995	-0.047475	2.869481
247.274518	2683.733717	17.584000	-0.047457	2.865560
247.061463	2675.782455	17.589005	-0.047412	2.861634
247.016964	2667.824605	17.594010	-0.047399	2.857707
247.139105	2659.786981	17.599015	-0.047416	2.853745
247.126069	2651.792055	17.604019	-0.047409	2.849792
246.964862	2643.870286	17.609024	-0.047373	2.845861
246.904248	2635.898493	17.614029	-0.047357	2.841905
246.818207	2627.960813	17.619034	-0.047336	2.837959
246.749842	2619.943117	17.624039	-0.047318	2.833969
246.989388	2611.887424	17.629043	-0.047357	2.829971
246.766840	2603.946152	17.634048	-0.047310	2.825999
246.621239	2595.996789	17.639053	-0.047278	2.822022
246.580397	2588.027431	17.644058	-0.047265	2.818034
246.504700	2580.023509	17.649063	-0.047246	2.814022
246.422783	2572.037977	17.654067	-0.047225	2.810013
246.205625	2564.098638	17.659072	-0.047180	2.806014
246.280293	2556.113673	17.664077	-0.047188	2.802003
246.482535	2548.132252	17.669082	-0.047221	2.797995
246.276330	2540.154745	17.674087	-0.047177	2.793960
246.240264	2532.153194	17.679091	-0.047165	2.789917
246.153757	2524.191294	17.684096	-0.047144	2.785885
246.131137	2516.202779	17.689101	-0.047134	2.781837
245.985719	2508.261049	17.694106	-0.047102	2.777800
245.934839	2500.277592	17.699111	-0.047087	2.773741
245.866714	2492.288844	17.704115	-0.047069	2.769673
245.919655	2484.313685	17.709120	-0.047074	2.765613
245.768242	2476.355714	17.714125	-0.047040	2.761543
245.846616	2468.404675	17.719130	-0.047050	2.757485
245.712219	2460.375602	17.724135	-0.047019	2.753368
245.772782	2452.326008	17.729139	-0.047025	2.749246
245.784782	2444.364051	17.734144	-0.047022	2.745160
245.482982	2436.430839	17.739149	-0.046961	2.741064
245.472432	2428.481992	17.744154	-0.046954	2.736971
245.323190	2420.494859	17.749159	-0.046921	2.732843
245.312423	2412.495645	17.754163	-0.046913	2.728712
245.096986	2404.543652	17.759168	-0.046868	2.724586
245.136238	2396.572402	17.764173	-0.046870	2.720460
245.216899	2388.611909	17.769178	-0.046880	2.716336
245.111545	2380.623153	17.774183	-0.046855	2.712179
244.963232	2372.662616	17.779187	-0.046822	2.708027
244.949131	2364.680383	17.784192	-0.046814	2.703867
244.906317	2356.697739	17.789197	-0.046801	2.699697
244.854481	2348.763142	17.794202	-0.046786	2.695546
244.818425	2340.720924	17.799207	-0.046774	2.691334
245.007688	2332.757635	17.804211	-0.046804	2.687170
244.850547	2324.804327	17.809216	-0.046770	2.682983
244.648239	2316.858887	17.814221	-0.046727	2.678791
244.614971	2308.896108	17.819226	-0.046715	2.674593
244.512995	2300.877893	17.824231	-0.046691	2.670356
244.478384	2292.902076	17.829235	-0.046679	2.666138
244.298581	2284.956518	17.834240	-0.046641	2.661921
244.195299	2276.989641	17.839245	-0.046616	2.657690
244.271898	2269.014192	17.844250	-0.046625	2.653460
244.106747	2261.014036	17.849255	-0.046589	2.649194
244.141808	2253.050126	17.854259	-0.046590	2.644954
244.130553	2245.100539	17.859264	-0.046583	2.640711
244.130795	2237.122049	17.864269	-0.046578	2.636447
243.989748	2229.144085	17.869274	-0.046546	2.632167
243.920644	2221.142991	17.874279	-0.046528	2.627872
243.966881	2213.182051	17.879283	-0.046532	2.623599
243.894528	2205.240845	17.884288	-0.046513	2.619322
243.748558	2197.269637	17.889293	-0.046480	2.615017
243.715453	2189.290164	17.894298	-0.046469	2.610709
243.783716	2181.308725	17.899303	-0.046476	2.606398
243.680311	2173.362035	17.904307	-0.046452	2.602088
243.639942	2165.422174	17.909312	-0.046439	2.597778
243.441886	2157.377057	17.914317	-0.046397	2.593394
243.493828	2149.275806	17.919322	-0.046401	2.588988
243.446657	2141.317981	17.924327	-0.046387	2.584647
243.321727	2133.428402	17.929331	-0.046359	2.580330
243.278395	2125.489126	17.934336	-0.046346	2.575984
243.259691	2117.504390	17.939341	-0.046337	2.571607
243.135086	2109.551958	17.944346	-0.046308	2.567234
243.093926	2101.590733	17.949351	-0.046296	2.562854
243.169426	2093.645144	17.954355	-0.046304	2.558483
243.063198	2085.696725	17.959360	-0.046279	2.554091
243.032489	2077.691251	17.964365	-0.046268	2.549664
243.033528	2069.732016	17.969370	-0.046263	2.545258
242.668556	2061.801190	17.974375	-0.046190	2.540834
242.738951	2053.831910	17.979379	-0.046198	2.536412
242.760347	2045.857490	17.984384	-0.046197	2.531975
242.517721	2037.896811	17.989389	-0.046146	2.527520
242.548283	2029.938357	17.994394	-0.046147	2.523078
242.492749	2021.967262	17.999399	-0.046131	2.518614
242.647953	2013.974175	18.004403	-0.046155	2.514146
242.469408	2006.006028	18.009408	-0.046116	2.509659
242.344426	1998.026505	18.014413	-0.046088	2.505162
242.363334	1990.081633	18.019418	-0.046086	2.500686
242.368210	1982.126526	18.024423	-0.046082	2.496196
242.105092	1974.167053	18.029427	-0.046027	2.491676
242.108851	1966.201757	18.034432	-0.046023	2.487163
242.198616	1958.215055	18.039437	-0.046034	2.482637
241.963596	1950.319208	18.044442	-0.045985	2.478130
241.744910	1942.352244	18.049447	-0.045939	2.473575
241.858540	1934.336143	18.054451	-0.045955	2.469009
241.912221	1926.351595	18.059456	-0.045960	2.464448
241.682331	1918.442153	18.064461	-0.045912	2.459900
242.042678	1910.453604	18.069466	-0.045974	2.455342
241.687551	1902.502089	18.074471	-0.045903	2.450744
241.400195	1894.573902	18.079475	-0.045844	2.446156
241.338614	1886.623876	18.084480	-0.045827	2.441563
241.301376	1878.642490	18.089485	-0.045815	2.436945
241.349854	1870.647751	18.094490	-0.045819	2.432317
241.202110	1862.644584	18.099495	-0.045786	2.427661
241.256738	1854.681397	18.104499	-0.045791	2.423034
241.003130	1846.766851	18.109504	-0.045738	2.418403
241.002942	1838.799110	18.114509	-0.045733	2.413752
240.939706	1830.843071	18.119514	-0.045716	2.409094
240.830696	1822.865946	18.124519	-0.045691	2.404410
240.942157	1814.907809	18.129523	-0.045706	2.399746
240.969782	1806.972770	18.134528	-0.045706	2.395080
240.900765	1798.984028	18.139533	-0.045688	2.390366
240.835101	1791.040472	18.144538	-0.045670	2.385669
240.478332	1783.123552	18.149543	-0.045599	2.380955
240.685566	1775.145495	18.154547	-0.045632	2.376241
240.692894	1767.178415	18.159552	-0.045628	2.371508
240.299653	1759.255305	18.164557	-0.045550	2.366759
240.367145	1751.292185	18.169562	-0.045557	2.362014
240.422358	1743.326576	18.174567	-0.045562	2.357257
240.298477	1735.361822	18.179571	-0.045534	2.352477
240.064519	1727.409478	18.184576	-0.045485	2.347685
240.036872	1719.435260	18.189581	-0.045475	2.342887
240.287966	1711.470711	18.194586	-0.045516	2.338108
240.024941	1703.537207	18.199591	-0.045462	2.333295
240.027770	1695.568174	18.204595	-0.045457	2.328473
239.915943	1687.639964	18.209600	-0.045431	2.323656
239.743440	1679.696996	18.214605	-0.045394	2.318815
239.682478	1671.749882	18.219610	-0.045377	2.313971
239.804875	1663.750965	18.224615	-0.045395	2.309100
239.648358	1655.814101	18.229619	-0.045360	2.304234
239.571609	1647.886486	18.234624	-0.045341	2.299370
239.632978	1639.913585	18.239629	-0.045347	2.294479
239.554016	1631.967013	18.244634	-0.045327	2.289582
239.236798	1624.037622	18.249639	-0.045263	2.284664
239.189857	1616.104191	18.254643	-0.045249	2.279757
239.163046	1608.160164	18.259648	-0.045239	2.274834
238.983854	1600.114710	18.264653	-0.045200	2.269825
238.940154	1592.168402	18.269658	-0.045187	2.264878
238.942500	1584.225096	18.274663	-0.045182	2.259925
238.793969	1576.296896	18.279667	-0.045149	2.254958
238.830758	1568.333385	18.284672	-0.045150	2.249975
238.832311	1560.354614	18.289677	-0.045146	2.244967
238.799600	1552.449714	18.294682	-0.045134	2.239992
238.519543	1544.539487	18.299687	-0.045077	2.234980
238.547694	1536.551345	18.304691	-0.045077	2.229936
238.721840	1528.572900	18.309696	-0.045104	2.224898
238.535127	1520.655290	18.314701	-0.045064	2.219856
238.558706	1512.730961	18.319706	-0.045063	2.214817
238.466362	1504.760456	18.324711	-0.045041	2.209727
238.355957	1496.829936	18.329715	-0.045015	2.204649
238.377638	1488.901593	18.334720	-0.045014	2.199572
238.138553	1480.977040	18.339725	-0.044964	2.194462
238.080572	1473.008952	18.344730	-0.044948	2.189329
237.897593	1465.064918	18.349735	-0.044909	2.184188
237.816311	1457.137366	18.354739	-0.044888	2.179055
237.936275	1449.175234	18.359744	-0.044905	2.173905
237.789991	1441.226215	18.364749	-0.044873	2.168727
237.957367	1433.273476	18.369754	-0.044899	2.163564
237.767970	1425.366952	18.374759	-0.044858	2.158385
237.772479	1417.419247	18.379763	-0.044854	2.153185
237.647843	1409.475637	18.384768	-0.044826	2.147963
237.654489	1401.523647	18.389773	-0.044822	2.142735
237.785493	1393.580817	18.394778	-0.044841	2.137512
237.625649	1385.651533	18.399783	-0.044806	2.132257
237.374540	1377.741573	18.404787	-0.044754	2.126994
237.450018	1369.809603	18.409792	-0.044763	2.121734
237.287547	1361.889539	18.414797	-0.044727	2.116446
237.240061	1353.887303	18.419802	-0.044713	2.111101
237.082073	1345.943892	18.424807	-0.044678	2.105771
237.093545	1338.005510	18.429811	-0.044675	2.100447
237.008126	1330.092197	18.434816	-0.044654	2.095118
236.917186	1322.147141	18.439821	-0.044632	2.089752
236.831378	1314.232632	18.444826	-0.044611	2.084394
236.910910	1306.295183	18.449831	-0.044620	2.079023
236.640726	1298.401023	18.454835	-0.044565	2.073633
236.678489	1290.436047	18.459840	-0.044567	2.068211
236.720557	1282.476214	18.464845	-0.044569	2.062779
236.519705	1274.601216	18.469850	-0.044527	2.057366
236.525854	1266.649152	18.474855	-0.044523	2.051907
236.619282	1258.678726	18.479859	-0.044535	2.046429
236.360177	1250.807640	18.484864	-0.044481	2.040970
236.272690	1242.886432	18.489869	-0.044460	2.035478
236.287836	1234.916306	18.494874	-0.044457	2.029948
236.040998	1227.006188	18.499879	-0.044406	2.024418
235.939433	1219.102704	18.504883	-0.044382	2.018893
235.922635	1211.172538	18.509888	-0.044374	2.013342
235.823830	1203.221249	18.514893	-0.044350	2.007752
235.866031	1195.305858	18.519898	-0.044353	2.002187
235.555102	1187.420975	18.524903	-0.044290	1.996591
235.659887	1179.454248	18.529907	-0.044304	1.990965
235.781356	1171.511186	18.534912	-0.044321	1.985342
235.568532	1163.613488	18.539917	-0.044276	1.979699
235.582453	1155.708840	18.544922	-0.044274	1.974060
235.644526	1147.744641	18.549927	-0.044280	1.968366
235.490771	1139.856904	18.554931	-0.044246	1.962688
235.303724	1131.974763	18.559936	-0.044206	1.956994
235.175187	1124.007830	18.564941	-0.044177	1.951228
235.016185	1116.092335	18.569946	-0.044142	1.945480
235.078332	1108.151917	18.574951	-0.044149	1.939720
234.967870	1100.252804	18.579955	-0.044123	1.933954
235.020604	1092.306889	18.584960	-0.044127	1.928154
234.807580	1084.414201	18.589965	-0.044083	1.922347
234.745070	1076.534895	18.594970	-0.044066	1.916549
234.741832	1068.600316	18.599975	-0.044060	1.910699
234.692814	1060.676275	18.604979	-0.044046	1.904833
234.762813	1052.782582	18.609984	-0.044053	1.898986
234.721091	1044.855060	18.614989	-0.044040	1.893082
234.583506	1036.965565	18.619994	-0.044010	1.887177
234.396801	1029.068346	18.624999	-0.043970	1.881243
234.285425	1021.175994	18.630003	-0.043944	1.875302
234.374196	1013.233543	18.635008	-0.043955	1.869327
234.344156	1005.306457	18.640013	-0.043944	1.863331
234.375591	997.413159	18.645018	-0.043945	1.857349
234.239652	989.509990	18.650023	-0.043914	1.851320
234.126131	981.616555	18.655027	-0.043888	1.845281
233.927904	973.762618	18.660032	-0.043846	1.839243
233.979600	965.836408	18.665037	-0.043850	1.833159
233.808359	957.952299	18.670042	-0.043813	1.827061
233.665146	950.054047	18.675047	-0.043781	1.820934
233.707595	942.150040	18.680051	-0.043784	1.814805
233.650178	934.252844	18.685056	-0.043768	1.808648
233.520765	926.363956	18.690061	-0.043739	1.802468
233.339756	918.508392	18.695066	-0.043700	1.796286
233.405465	910.530678	18.700071	-0.043707	1.790017
233.097830	902.662969	18.705075	-0.043645	1.783767
233.180764	894.763815	18.710080	-0.043655	1.777518
233.223705	886.846602	18.715085	-0.043658	1.771228
233.065890	878.988475	18.720090	-0.043623	1.764938
232.739610	871.152223	18.725095	-0.043557	1.758621
232.906936	863.224721	18.730099	-0.043583	1.752270
232.907353	855.331157	18.735104	-0.043578	1.745903
232.641494	847.477577	18.740109	-0.043523	1.739511
232.592782	839.608328	18.745114	-0.043509	1.733110
232.649901	831.696918	18.750119	-0.043514	1.726664
232.545336	823.830997	18.755123	-0.043490	1.720211
232.328523	816.002614	18.760128	-0.043444	1.713750
232.116608	808.107379	18.765133	-0.043400	1.707210
232.260342	800.199125	18.770138	-0.043421	1.700680
232.274990	792.322478	18.775143	-0.043419	1.694134
232.204457	784.437565	18.780147	-0.043400	1.687545
232.141455	776.594359	18.785152	-0.043383	1.680966
231.906692	768.756077	18.790157	-0.043335	1.674343
231.866506	760.872392	18.795162	-0.043322	1.667680
231.894259	752.990296	18.800167	-0.043322	1.661002
231.599945	745.167562	18.805171	-0.043262	1.654303
231.770353	737.265635	18.810176	-0.043288	1.647573
231.610988	729.419966	18.815181	-0.043254	1.640818
231.738027	721.543316	18.820186	-0.043272	1.634048
231.345078	713.679162	18.825191	-0.043194	1.627188
231.214515	705.826827	18.830195	-0.043164	1.620347
231.292324	697.962596	18.835200	-0.043174	1.613495
231.028481	690.124335	18.840205	-0.043119	1.606588
230.945193	682.294563	18.845210	-0.043099	1.599685
231.003580	674.432682	18.850215	-0.043104	1.592743
231.105613	666.548448	18.855219	-0.043118	1.585758
230.932146	658.746269	18.860224	-0.043081	1.578775
230.715697	650.911406	18.865229	-0.043035	1.571725
230.907908	643.041229	18.870234	-0.043066	1.564672
230.757429	635.231637	18.875239	-0.043033	1.557591
230.608995	627.388020	18.880243	-0.043000	1.550447
230.783907	619.524173	18.885248	-0.043027	1.543299
230.634504	611.702671	18.890253	-0.042994	1.536109
230.555075	603.882160	18.895258	-0.042974	1.528896
230.445850	596.063674	18.900263	-0.042949	1.521647
230.416867	588.250330	18.905267	-0.042938	1.514379
229.950448	580.482347	18.910272	-0.042846	1.507052
229.913798	572.643511	18.915277	-0.042834	1.499689
230.093506	564.797723	18.920282	-0.042863	1.492316
229.984876	556.981524	18.925287	-0.042837	1.484890
229.748005	549.214170	18.930291	-0.042788	1.477453
229.748420	541.354704	18.935296	-0.042783	1.469927
229.599646	533.540931	18.940301	-0.042750	1.462383
229.543091	525.753054	18.945306	-0.042734	1.454840
229.417759	517.944639	18.950311	-0.042706	1.447226
229.304069	510.166846	18.955315	-0.042680	1.439604
229.262575	502.379887	18.960320	-0.042667	1.431944
229.076011	494.584425	18.965325	-0.042627	1.424210
229.106660	486.795857	18.970330	-0.042627	1.416477
228.918154	479.023734	18.975335	-0.042587	1.408682
228.848053	471.239977	18.980339	-0.042569	1.400851
228.871760	463.466133	18.985344	-0.042568	1.393001
228.785720	455.662845	18.990349	-0.042547	1.385059
228.669218	447.913930	18.995354	-0.042520	1.377122
228.252437	440.189390	19.000359	-0.042438	1.369112
228.307271	432.395965	19.005363	-0.042443	1.361064
228.301722	424.646214	19.010368	-0.042437	1.353004
228.151110	416.874486	19.015373	-0.042403	1.344847
228.239103	409.120824	19.020378	-0.042415	1.336702
228.035908	401.383731	19.025383	-0.042372	1.328472
227.672411	393.693960	19.030387	-0.042299	1.320213
227.941673	385.853353	19.035392	-0.042344	1.311854
227.808926	378.052510	19.040397	-0.042314	1.303411
227.647708	370.354507	19.045402	-0.042279	1.295020
227.589559	362.621604	19.050407	-0.042263	1.286555
227.510291	354.919600	19.055411	-0.042243	1.278063
227.457553	347.216367	19.060416	-0.042228	1.269519
227.298897	339.516384	19.065421	-0.042194	1.260900
227.441822	331.794322	19.070426	-0.042215	1.252255
227.129892	324.135410	19.075431	-0.042152	1.243534
226.802169	316.490446	19.080435	-0.042086	1.234763
226.836279	308.764597	19.085440	-0.042087	1.225908
226.664631	301.097533	19.090445	-0.042050	1.217016
226.567937	293.426599	19.095450	-0.042027	1.208068
226.291100	285.793939	19.100455	-0.041971	1.199063
226.320476	278.107085	19.105459	-0.041971	1.189987
226.161824	270.465849	19.110464	-0.041937	1.180858
226.019056	262.822257	19.115469	-0.041905	1.171657
225.788368	255.204483	19.120474	-0.041857	1.162397
225.699498	247.562216	19.125479	-0.041835	1.153062
225.434725	239.926089	19.130483	-0.041781	1.143622
225.223491	232.334008	19.135488	-0.041737	1.134168
225.137395	224.700208	19.140493	-0.041716	1.124610
225.103401	217.102068	19.145498	-0.041704	1.115027
224.733823	209.532655	19.150503	-0.041631	1.105323
224.580524	201.960099	19.155507	-0.041597	1.095577
224.204793	194.416144	19.160512	-0.041522	1.085730
223.721367	186.907548	19.165517	-0.041427	1.075816
223.611392	179.326078	19.170522	-0.041402	1.065798
223.036380	171.846480	19.175527	-0.041290	1.055713
222.560749	164.341473	19.180531	-0.041196	1.045520
222.319602	156.833916	19.185536	-0.041146	1.035278
221.868462	149.341183	19.190541	-0.041057	1.024904
221.412707	141.883487	19.195546	-0.040968	1.014471
220.913409	134.430040	19.200551	-0.040870	1.003925
220.550178	126.959733	19.205555	-0.040797	0.993276
220.277209	119.472198	19.210560	-0.040741	0.982510
219.605939	112.080244	19.215565	-0.040612	0.971662
219.126934	104.674765	19.220570	-0.040517	0.960721
218.633819	97.277292	19.225575	-0.040421	0.949661
218.092187	89.905188	19.230579	-0.040315	0.938497
217.662465	82.532117	19.235584	-0.040230	0.927226
217.077239	75.205308	19.240589	-0.040116	0.915845
216.520720	67.876228	19.245594	-0.040008	0.904325
215.968065	60.798121	19.250599	-0.039900	0.893054