Tue Mar 23 10:33:24 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.501769	0.030985	0.000000	0.000026	0.720228

0.476213	0.030452	0.005005	0.000031	0.720218
0.380424	0.051732	0.010010	0.000049	0.720226
0.312508	0.060761	0.015014	0.000061	0.720220
0.588540	0.011599	0.020019	0.000010	0.720220
0.701825	-0.006723	0.025024	-0.000011	0.720224
0.631828	0.002755	0.030029	0.000002	0.720218
0.640315	0.007093	0.035034	0.000001	0.720229
0.546420	0.019836	0.040038	0.000018	0.720221
0.389780	0.049535	0.045043	0.000047	0.720224
0.652458	0.003900	0.050048	-0.000001	0.720226
0.354069	0.053766	0.055053	0.000054	0.720220
0.660984	0.004296	0.060058	-0.000003	0.720230
0.561779	-0.127644	0.065062	0.000016	0.719935
0.579927	-0.148390	0.070067	0.000013	0.719900
0.576800	-0.146184	0.075072	0.000013	0.719904
0.395059	-0.119579	0.080077	0.000047	0.719892
0.691873	-0.166898	0.085082	-0.000008	0.719903
0.762846	-0.181766	0.090086	-0.000021	0.719898
0.687238	-0.168238	0.095091	-0.000007	0.719898
0.634742	-0.221816	0.100096	0.000003	0.719774
0.641237	-0.313276	0.105101	0.000002	0.719596
0.665952	-0.311160	0.110106	-0.000003	0.719609
0.441319	-0.275530	0.115110	0.000039	0.719600
0.563745	-0.296748	0.120115	0.000016	0.719601
0.582585	-0.304826	0.125120	0.000013	0.719591
0.420770	-0.441624	0.130125	0.000043	0.719265
0.518914	-0.453892	0.135130	0.000025	0.719275
0.506369	-0.453531	0.140134	0.000027	0.719271
0.525933	-0.456949	0.145139	0.000024	0.719271
0.621308	-0.555629	0.150144	0.000006	0.719110
0.416424	-0.598333	0.155149	0.000044	0.718953
0.467260	-0.602061	0.160154	0.000035	0.718964
0.315224	-0.577928	0.165158	0.000063	0.718958
0.508948	-0.698473	0.170163	0.000027	0.718788
0.555214	-0.780093	0.175168	0.000019	0.718643
0.618920	-0.795245	0.180173	0.000007	0.718635
0.598699	-0.800630	0.185178	0.000011	0.718617
0.618976	-0.940313	0.190182	0.000007	0.718348
0.530398	-0.924315	0.195187	0.000024	0.718349
0.480824	-0.911827	0.200192	0.000033	0.718356
0.381175	-1.055300	0.205197	0.000052	0.718037
0.465405	-1.078725	0.210202	0.000036	0.718020
0.388293	-1.068995	0.215206	0.000051	0.718012
0.667472	-1.262879	0.220211	-0.000001	0.717727
0.640515	-1.270408	0.225216	0.000004	0.717703
0.273258	-1.234664	0.230221	0.000073	0.717644
0.371641	-1.385190	0.235226	0.000054	0.717381
0.420624	-1.395781	0.240230	0.000045	0.717377
0.303393	-1.448574	0.245235	0.000067	0.717231
0.276086	-1.514921	0.250240	0.000072	0.717090
0.010866	-1.472868	0.255245	0.000122	0.717080
0.211581	-1.650306	0.260250	0.000085	0.716799
0.217007	-1.672101	0.265254	0.000084	0.716758
0.197120	-1.737397	0.270259	0.000088	0.716621
0.236648	-1.830718	0.275264	0.000080	0.716450
0.119866	-1.827744	0.280269	0.000102	0.716415
-0.038765	-1.940422	0.285274	0.000132	0.716135
0.093943	-1.965449	0.290278	0.000107	0.716132
-0.006808	-2.045659	0.295283	0.000126	0.715938
-0.226133	-2.031337	0.300288	0.000167	0.715889
-0.272853	-2.112712	0.305293	0.000176	0.715711
-0.119614	-2.221374	0.310298	0.000147	0.715549
-0.313351	-2.235796	0.315302	0.000184	0.715452
-0.793611	-2.261808	0.320307	0.000273	0.715231
-1.300333	-2.167831	0.325312	0.000367	0.715238
-2.098147	-2.188834	0.330317	0.000516	0.714914
-2.424680	-2.130372	0.335322	0.000577	0.714914
-2.494614	-2.146591	0.340326	0.000590	0.714857
-3.254881	-2.136499	0.345331	0.000732	0.714608
-3.057598	-2.168626	0.350336	0.000695	0.714614
-3.508275	-2.102630	0.355341	0.000779	0.714586
-3.882003	-2.190407	0.360346	0.000849	0.714279
-4.094137	-2.153459	0.365350	0.000888	0.714277
-4.226109	-2.132282	0.370355	0.000913	0.714273
-4.131051	-2.253464	0.375360	0.000895	0.714065
-5.480137	-2.064175	0.380365	0.001146	0.713964
-5.075402	-2.132081	0.385370	0.001071	0.713972
-4.858616	-2.171417	0.390374	0.001031	0.713970
-5.969747	-2.121967	0.395379	0.001238	0.713675
-6.096822	-2.108410	0.400384	0.001262	0.713657
-6.117882	-2.106987	0.405389	0.001266	0.713652
-5.896794	-2.143164	0.410394	0.001224	0.713658
-6.261971	-2.150685	0.415398	0.001293	0.713514
-7.013733	-2.092816	0.420403	0.001433	0.713362
-6.741043	-2.140660	0.425408	0.001382	0.713364
-7.193742	-2.063679	0.430413	0.001466	0.713356
-7.041883	-2.086977	0.435418	0.001438	0.713364
-7.303728	-2.161423	0.440422	0.001487	0.713123
-8.395825	-2.017042	0.445427	0.001690	0.713023
-7.738203	-2.131969	0.450432	0.001568	0.713027
-7.588147	-2.161928	0.455437	0.001540	0.713020
-7.959300	-2.091785	0.460442	0.001609	0.713028
-7.876803	-2.176162	0.465446	0.001594	0.712889
-8.755987	-2.109980	0.470451	0.001758	0.712709
-8.452768	-2.157973	0.475456	0.001701	0.712721
-9.022155	-2.062275	0.480461	0.001807	0.712709
-8.915012	-2.079376	0.485466	0.001787	0.712713
-8.525066	-2.150893	0.490470	0.001715	0.712709
-9.484089	-2.124017	0.495475	0.001894	0.712422
-9.663931	-2.107583	0.500480	0.001927	0.712391
-9.716373	-2.103659	0.505485	0.001937	0.712380
-9.712937	-2.098760	0.510490	0.001936	0.712391
-9.640324	-2.113433	0.515494	0.001923	0.712387
-9.820932	-2.081388	0.520499	0.001957	0.712387
-9.628960	-2.212029	0.525504	0.001921	0.712195
-10.814515	-2.056517	0.530509	0.002142	0.712083
-10.450675	-2.117981	0.535514	0.002074	0.712090
-10.488668	-2.113143	0.540518	0.002081	0.712086
-11.056289	-2.012386	0.545523	0.002187	0.712085
-10.511424	-2.105865	0.550528	0.002086	0.712092
-10.384072	-2.182870	0.555533	0.002062	0.711984
-11.624556	-2.072072	0.560538	0.002293	0.711764
-11.734432	-2.054623	0.565542	0.002313	0.711759
-11.851647	-2.034457	0.570547	0.002335	0.711758
-11.322047	-2.125886	0.575552	0.002237	0.711764
-11.541309	-2.091415	0.580557	0.002278	0.711754
-11.642383	-2.070016	0.585562	0.002297	0.711761
-11.481228	-2.167690	0.590566	0.002267	0.711623
-12.706073	-2.035987	0.595571	0.002495	0.711451
-12.044919	-2.150544	0.600576	0.002372	0.711457
-12.269990	-2.115113	0.605581	0.002414	0.711447
-12.362198	-2.093965	0.610586	0.002431	0.711457
-12.463562	-2.077835	0.615590	0.002450	0.711453
-12.486492	-2.074584	0.620595	0.002454	0.711451
-12.297298	-2.234007	0.625600	0.002419	0.711200
-13.860703	-1.989380	0.630605	0.002710	0.711132
-13.581668	-2.036526	0.635610	0.002658	0.711137
-12.901160	-2.159696	0.640614	0.002532	0.711133
-13.421683	-2.067869	0.645619	0.002629	0.711131
-13.255286	-2.092250	0.650624	0.002598	0.711142
-13.193873	-2.106996	0.655629	0.002586	0.711134
-13.584210	-2.156621	0.660634	0.002659	0.710896
-14.368411	-2.030086	0.665638	0.002805	0.710869
-14.475628	-2.013459	0.670643	0.002825	0.710864
-13.839971	-2.121761	0.675648	0.002707	0.710874
-14.332329	-2.039992	0.680653	0.002799	0.710862
-14.034442	-2.088740	0.685658	0.002743	0.710870
-13.778929	-2.153037	0.690662	0.002696	0.710833
-14.972580	-2.093000	0.695667	0.002918	0.710528
-14.695849	-2.137825	0.700672	0.002867	0.710537
-15.153300	-2.059927	0.705677	0.002952	0.710529
-14.896030	-2.102145	0.710682	0.002904	0.710536
-15.122940	-2.062666	0.715686	0.002946	0.710534
-15.354081	-2.023957	0.720691	0.002990	0.710529
-14.828126	-2.148032	0.725696	0.002892	0.710469
-16.221346	-2.028883	0.730701	0.003151	0.710210
-15.948602	-2.071478	0.735706	0.003100	0.710222
-16.054035	-2.055594	0.740710	0.003120	0.710216
-16.119064	-2.045465	0.745715	0.003132	0.710213
-16.119893	-2.041152	0.750720	0.003133	0.710221
-16.317332	-2.011296	0.755725	0.003169	0.710211
-15.911818	-2.078836	0.760730	0.003094	0.710220
-16.151742	-2.135695	0.765734	0.003139	0.710021
-17.454220	-1.970065	0.770739	0.003381	0.709888
-16.472181	-2.140296	0.775744	0.003199	0.709897
-16.714920	-2.100765	0.780749	0.003244	0.709890
-17.017513	-2.044480	0.785754	0.003300	0.709894
-16.549402	-2.128135	0.790758	0.003213	0.709894
-17.001901	-2.048653	0.795763	0.003297	0.709891
-17.121027	-2.123318	0.800768	0.003320	0.709699
-17.895268	-2.040969	0.805773	0.003464	0.709588
-17.544264	-2.099273	0.810778	0.003399	0.709596
-17.913962	-2.033996	0.815782	0.003468	0.709595
-18.177326	-1.988993	0.820787	0.003517	0.709591
-17.350580	-2.133197	0.825792	0.003363	0.709597
-17.766573	-2.062675	0.830797	0.003440	0.709590
-18.103522	-2.094233	0.835802	0.003503	0.709406
-18.732732	-2.054155	0.840806	0.003620	0.709262
-18.594888	-2.079392	0.845811	0.003595	0.709260
-18.607624	-2.074211	0.850816	0.003597	0.709266
-18.935006	-2.019241	0.855821	0.003658	0.709259
-18.332292	-2.124895	0.860826	0.003546	0.709263
-18.456256	-2.104729	0.865830	0.003569	0.709259
-18.961327	-2.096850	0.870835	0.003663	0.709094
-19.558469	-2.059878	0.875840	0.003775	0.708955
-19.549689	-2.065040	0.880845	0.003773	0.708948
-19.610244	-2.051222	0.885850	0.003784	0.708953
-19.423989	-2.084073	0.890854	0.003750	0.708954
-19.348584	-2.099315	0.895859	0.003736	0.708950
-19.611753	-2.048301	0.900864	0.003785	0.708958
-19.763840	-2.079747	0.905869	0.003813	0.708841
-20.275722	-2.089924	0.910874	0.003909	0.708638
-20.410227	-2.066124	0.915878	0.003934	0.708637
-20.878704	-1.984798	0.920883	0.004021	0.708633
-20.310655	-2.082684	0.925888	0.003915	0.708639
-20.399476	-2.070453	0.930893	0.003932	0.708632
-20.644350	-2.023557	0.935898	0.003978	0.708638
-20.450403	-2.078503	0.940902	0.003942	0.708597
-21.081562	-2.091569	0.945907	0.004059	0.708346
-20.981052	-2.105131	0.950912	0.004041	0.708354
-21.564245	-2.005074	0.955917	0.004149	0.708346
-21.025632	-2.098691	0.960922	0.004049	0.708351
-21.189060	-2.071177	0.965926	0.004079	0.708348
-21.592429	-2.000555	0.970931	0.004155	0.708345
-21.249409	-2.104446	0.975936	0.004091	0.708259
-22.500075	-2.008605	0.980941	0.004324	0.708004
-22.546669	-1.997901	0.985946	0.004332	0.708009
-22.424175	-2.018069	0.990950	0.004310	0.708012
-22.074663	-2.081221	0.995955	0.004245	0.708010
-21.975387	-2.094955	1.000960	0.004226	0.708018
-22.571158	-1.994131	1.005965	0.004337	0.708007
-22.404940	-2.020572	1.010970	0.004306	0.708014
-22.414175	-2.131477	1.015974	0.004308	0.707788
-23.615756	-1.963966	1.020979	0.004532	0.707694
-23.000599	-2.068702	1.025984	0.004418	0.707704
-22.645900	-2.137254	1.030989	0.004352	0.707693
-23.170921	-2.038530	1.035994	0.004449	0.707703
-23.246857	-2.026993	1.040998	0.004464	0.707699
-23.177910	-2.041199	1.046003	0.004451	0.707695
-23.493316	-2.096710	1.051008	0.004510	0.707471
-24.476167	-1.971419	1.056013	0.004693	0.707370
-24.112845	-2.033768	1.061018	0.004625	0.707375
-23.802106	-2.091568	1.066022	0.004567	0.707370
-24.510917	-1.964135	1.071027	0.004699	0.707372
-24.149989	-2.025435	1.076032	0.004632	0.707378
-23.835419	-2.086717	1.081037	0.004574	0.707368
-24.225443	-2.059447	1.086042	0.004646	0.707283
-24.975900	-2.025541	1.091046	0.004786	0.707082
-24.671312	-2.083916	1.096051	0.004730	0.707074
-24.988531	-2.021759	1.101056	0.004789	0.707085
-25.102417	-2.005672	1.106061	0.004810	0.707076
-25.077379	-2.008553	1.111066	0.004805	0.707079
-24.908608	-2.037516	1.116070	0.004774	0.707081
-25.212101	-2.004933	1.121075	0.004831	0.707038
-25.407287	-2.110428	1.126080	0.004867	0.706756
-25.799981	-2.046126	1.131085	0.004940	0.706745
-25.905825	-2.023507	1.136090	0.004960	0.706752
-25.731839	-2.054604	1.141094	0.004928	0.706752
-25.911640	-2.025680	1.146099	0.004961	0.706745
-25.918261	-2.020627	1.151104	0.004963	0.706753
-25.963529	-2.024692	1.156109	0.004971	0.706729
-26.240552	-2.118333	1.161114	0.005023	0.706441
-26.299806	-2.107668	1.166118	0.005034	0.706441
-26.967096	-1.992287	1.171123	0.005158	0.706434
-26.616559	-2.048055	1.176128	0.005093	0.706447
-26.406337	-2.089727	1.181133	0.005054	0.706439
-27.005932	-1.979772	1.186138	0.005165	0.706445
-26.785519	-2.051176	1.191142	0.005125	0.706380
-27.303645	-2.086946	1.196147	0.005221	0.706122
-27.076321	-2.121380	1.201152	0.005179	0.706134
-27.726392	-2.011742	1.206157	0.005300	0.706122
-27.551320	-2.039774	1.211162	0.005267	0.706128
-27.265517	-2.089520	1.216166	0.005214	0.706130
-27.893719	-1.981800	1.221171	0.005331	0.706122
-27.611225	-2.081679	1.226176	0.005279	0.706022
-28.314136	-2.037350	1.231181	0.005410	0.705859
-28.198490	-2.055452	1.236186	0.005388	0.705864
-28.285242	-2.041049	1.241190	0.005404	0.705861
-28.521261	-2.002875	1.246195	0.005448	0.705853
-28.048476	-2.079974	1.251200	0.005361	0.705868
-28.766611	-1.956299	1.256205	0.005494	0.705859
-28.688185	-2.054349	1.261210	0.005480	0.705690
-29.253775	-2.035964	1.266214	0.005585	0.705524
-29.126015	-2.061771	1.271219	0.005561	0.705517
-29.155562	-2.051592	1.276224	0.005567	0.705527
-29.301207	-2.030958	1.281229	0.005594	0.705516
-29.250679	-2.037339	1.286234	0.005585	0.705521
-29.575086	-1.978871	1.291238	0.005645	0.705523
-29.665421	-2.029082	1.296243	0.005662	0.705389
-30.141844	-2.031357	1.301248	0.005751	0.705213
-30.293120	-2.009289	1.306253	0.005779	0.705203
-30.437130	-1.978789	1.311258	0.005806	0.705213
-30.086881	-2.042778	1.316262	0.005741	0.705210
-30.362100	-1.996759	1.321267	0.005792	0.705203
-30.191204	-2.023820	1.326272	0.005761	0.705210
-30.158869	-2.055020	1.331277	0.005755	0.705159
-30.791004	-2.077512	1.336282	0.005872	0.704886
-30.925761	-2.051877	1.341286	0.005898	0.704889
-31.029237	-2.035924	1.346291	0.005917	0.704884
-30.651567	-2.099495	1.351296	0.005847	0.704892
-30.944870	-2.051218	1.356301	0.005901	0.704884
-31.430294	-1.962383	1.361306	0.005992	0.704888
-30.922607	-2.113431	1.366310	0.005897	0.704766
-31.989900	-2.014058	1.371315	0.006096	0.704583
-31.715306	-2.056316	1.376320	0.006045	0.704596
-32.179472	-1.977116	1.381325	0.006131	0.704589
-32.170251	-1.976642	1.386330	0.006130	0.704593
-31.816685	-2.040760	1.391334	0.006064	0.704591
-32.309299	-1.954940	1.396339	0.006156	0.704586
-31.940029	-2.057711	1.401344	0.006087	0.704512
-33.054719	-1.982364	1.406349	0.006295	0.704263
-32.939220	-2.002654	1.411354	0.006273	0.704263
-33.033744	-1.985391	1.416358	0.006291	0.704264
-32.968434	-2.000953	1.421363	0.006279	0.704256
-33.120974	-1.969401	1.426368	0.006307	0.704265
-33.231102	-1.952221	1.431373	0.006328	0.704260
-32.714655	-2.043361	1.436378	0.006232	0.704261
-33.115815	-2.077007	1.441382	0.006307	0.704049
-34.405074	-1.896029	1.446387	0.006547	0.703951
-33.731212	-2.011207	1.451392	0.006421	0.703960
-33.651258	-2.031390	1.456397	0.006407	0.703948
-34.282916	-1.914821	1.461402	0.006524	0.703956
-34.076378	-1.952771	1.466406	0.006486	0.703954
-33.877159	-1.990848	1.471411	0.006449	0.703948
-33.599321	-2.074930	1.476416	0.006397	0.703879
-34.570471	-2.024542	1.481421	0.006578	0.703631
-34.230875	-2.082344	1.486426	0.006515	0.703636
-34.657652	-2.006086	1.491430	0.006594	0.703636
-34.713688	-2.001639	1.496435	0.006605	0.703625
-34.279067	-2.072319	1.501440	0.006524	0.703639
-34.598135	-2.018084	1.506445	0.006584	0.703633
-34.827136	-2.088270	1.511450	0.006626	0.703409
-35.231028	-2.046085	1.516454	0.006702	0.703349
-35.309896	-2.035864	1.521459	0.006716	0.703341
-35.373535	-2.019584	1.526464	0.006728	0.703351
-35.883613	-1.933964	1.531469	0.006823	0.703340
-35.531869	-1.994127	1.536474	0.006758	0.703345
-35.127135	-2.071930	1.541478	0.006683	0.703333
-36.225113	-2.038929	1.546483	0.006887	0.703004
-36.228717	-2.033276	1.551488	0.006888	0.703014
-36.432228	-2.002224	1.556493	0.006926	0.703004
-36.421607	-2.003047	1.561498	0.006924	0.703006
-36.292206	-2.027208	1.566502	0.006900	0.703003
-36.592100	-1.976424	1.571507	0.006956	0.702998
-36.322163	-2.018955	1.576512	0.006906	0.703009
-37.095416	-2.028931	1.581517	0.007050	0.702710
-37.433335	-1.977158	1.586522	0.007113	0.702693
-37.086950	-2.037491	1.591526	0.007048	0.702696
-37.313071	-2.000629	1.596531	0.007090	0.702688
-37.071943	-2.039108	1.601536	0.007046	0.702697
-37.311686	-1.999586	1.606541	0.007090	0.702691
-37.131195	-2.030422	1.611546	0.007057	0.702693
-37.948703	-2.029232	1.616550	0.007209	0.702401
-38.295047	-1.984134	1.621555	0.007273	0.702367
-38.055403	-2.023511	1.626560	0.007229	0.702374
-38.127906	-2.013839	1.631565	0.007243	0.702367
-38.469149	-1.951549	1.636570	0.007306	0.702370
-38.359953	-1.970255	1.641574	0.007286	0.702371
-38.289471	-1.986383	1.646579	0.007273	0.702364
-37.987909	-2.112859	1.651584	0.007217	0.702217
-38.991266	-2.004755	1.656589	0.007404	0.702074
-38.960326	-2.010977	1.661594	0.007398	0.702072
-38.973880	-2.007608	1.666598	0.007401	0.702074
-39.192718	-1.970688	1.671603	0.007441	0.702069
-38.847938	-2.029312	1.676608	0.007377	0.702075
-39.057908	-1.996057	1.681613	0.007416	0.702066
-39.325683	-2.071831	1.686618	0.007466	0.701816
-39.661964	-2.047135	1.691622	0.007529	0.701745
-40.244924	-1.946223	1.696627	0.007638	0.701739
-39.830266	-2.015070	1.701632	0.007560	0.701749
-39.894037	-2.008841	1.706637	0.007572	0.701738
-40.032268	-1.982628	1.711642	0.007598	0.701741
-39.887232	-2.006029	1.716646	0.007571	0.701746
-40.221659	-2.058258	1.721651	0.007634	0.701520
-40.470407	-2.051810	1.726656	0.007680	0.701443
-40.865668	-1.985862	1.731661	0.007754	0.701433
-41.036305	-1.953254	1.736666	0.007785	0.701438
-40.674008	-2.016624	1.741670	0.007718	0.701440
-40.734386	-2.011267	1.746675	0.007729	0.701429
-40.632768	-2.022535	1.751680	0.007711	0.701443
-41.062275	-2.084191	1.756685	0.007791	0.701163
-41.674839	-1.995445	1.761690	0.007905	0.701121
-41.671516	-1.993892	1.766694	0.007904	0.701125
-41.652465	-2.002038	1.771699	0.007901	0.701115
-41.503557	-2.023282	1.776704	0.007873	0.701126
-41.936793	-1.949673	1.781709	0.007954	0.701119
-41.345984	-2.053247	1.786714	0.007844	0.701122
-41.727871	-2.103032	1.791718	0.007915	0.700883
-42.690084	-1.941385	1.796723	0.008094	0.700863
-42.600416	-1.951646	1.801728	0.008078	0.700874
-42.309148	-2.005821	1.806733	0.008023	0.700870
-42.369176	-1.993936	1.811738	0.008035	0.700872
-42.125357	-2.035724	1.816742	0.007989	0.700875
-42.373785	-2.053321	1.821747	0.008036	0.700749
-43.188523	-2.012891	1.826752	0.008187	0.700537
-43.177241	-2.017224	1.831757	0.008185	0.700532
-43.393287	-1.978830	1.836762	0.008226	0.700532
-43.154270	-2.018455	1.841766	0.008181	0.700538
-43.447203	-1.968508	1.846771	0.008236	0.700533
-43.099469	-2.027286	1.851776	0.008171	0.700539
-43.382166	-2.066870	1.856781	0.008224	0.700357
-44.309440	-1.969688	1.861786	0.008397	0.700218
-44.119468	-2.001648	1.866790	0.008361	0.700222
-44.154533	-1.997715	1.871795	0.008368	0.700217
-43.847080	-2.048660	1.876800	0.008311	0.700225
-44.171174	-1.995540	1.881805	0.008371	0.700215
-44.227742	-1.982041	1.886810	0.008382	0.700222
-44.279413	-2.091502	1.891814	0.008392	0.699981
-45.057428	-1.996590	1.896819	0.008536	0.699892
-44.917831	-2.016493	1.901824	0.008511	0.699902
-44.906710	-2.021756	1.906829	0.008509	0.699895
-45.027307	-1.999034	1.911834	0.008531	0.699897
-44.816216	-2.035222	1.916838	0.008492	0.699900
-44.998548	-2.014874	1.921843	0.008526	0.699875
-45.454116	-2.068860	1.926848	0.008611	0.699601
-45.713085	-2.025885	1.931853	0.008659	0.699594
-46.046403	-1.964733	1.936858	0.008721	0.699598
-45.425617	-2.071707	1.941862	0.008606	0.699605
-45.867406	-1.998286	1.946867	0.008688	0.699594
-46.093508	-1.953946	1.951872	0.008730	0.699602
-45.826498	-2.036619	1.956877	0.008680	0.699531
-46.595885	-2.028276	1.961882	0.008824	0.699269
-46.778833	-1.994628	1.966886	0.008858	0.699271
-47.160486	-1.928045	1.971891	0.008929	0.699268
-46.535526	-2.037689	1.976896	0.008813	0.699271
-46.807922	-1.988821	1.981901	0.008864	0.699272
-47.243763	-1.912039	1.986906	0.008945	0.699270
-46.803219	-1.989836	1.991910	0.008863	0.699271
-47.105528	-2.073751	1.996915	0.008919	0.698991
-47.788519	-1.966508	2.001920	0.009046	0.698961

-47.605462	-1.999173	2.011917	0.009012	0.698961
-47.553645	-2.008935	2.021914	0.009003	0.698959
-47.741833	-1.974632	2.031910	0.009038	0.698961
-47.501675	-2.016979	2.041907	0.008994	0.698961
-47.762424	-1.970467	2.051904	0.009042	0.698961
-47.328995	-2.048738	2.061901	0.008962	0.698959
-47.842847	-1.955979	2.071898	0.009057	0.698961
-47.511814	-2.015453	2.081894	0.008996	0.698960
-47.526177	-2.014722	2.091891	0.008999	0.698956
-47.538077	-2.009547	2.101888	0.009001	0.698962
-47.543154	-2.010778	2.111885	0.009002	0.698957
-47.735395	-1.974484	2.121882	0.009038	0.698961
-47.512841	-2.016075	2.131878	0.008997	0.698957
-47.331868	-1.985654	2.141875	0.008963	0.699084
-46.625826	-2.018192	2.151872	0.008832	0.699273
-46.648755	-2.013587	2.161869	0.008836	0.699274
-46.746867	-2.000654	2.171866	0.008855	0.699265
-46.774069	-1.996442	2.181862	0.008860	0.699263
-46.050780	-2.017984	2.191859	0.008725	0.699481
-45.798092	-2.005226	2.201856	0.008679	0.699598
-45.677523	-2.025670	2.211853	0.008656	0.699600
-45.801048	-2.004860	2.221850	0.008679	0.699597
-45.742510	-1.965749	2.231846	0.008669	0.699698
-44.835238	-2.030034	2.241843	0.008500	0.699895
-44.866577	-2.024469	2.251840	0.008506	0.699895
-44.936139	-2.010510	2.261837	0.008519	0.699898
-44.482108	-2.005310	2.271834	0.008434	0.700072
-44.101692	-2.001637	2.281830	0.008364	0.700217
-44.078286	-2.005101	2.291827	0.008360	0.700218
-44.132925	-1.993957	2.301824	0.008370	0.700221
-43.383927	-1.987667	2.311821	0.008231	0.700504
-43.215409	-2.001704	2.321818	0.008199	0.700537
-43.133955	-2.015634	2.331814	0.008184	0.700538
-43.089714	-1.981882	2.341811	0.008176	0.700622
-42.073978	-2.037097	2.351808	0.007987	0.700877
-41.985356	-2.051070	2.361805	0.007971	0.700880
-42.384947	-1.981006	2.371802	0.008045	0.700877
-42.014783	-1.993851	2.381798	0.007977	0.700985
-41.537675	-2.010941	2.391795	0.007888	0.701122
-41.567383	-2.004858	2.401792	0.007894	0.701124
-41.532183	-1.986662	2.411789	0.007887	0.701173
-40.861058	-1.977395	2.421786	0.007762	0.701434
-40.607822	-2.021988	2.431782	0.007715	0.701435
-40.750286	-1.995802	2.441779	0.007742	0.701436
-40.061863	-1.991843	2.451776	0.007614	0.701692
-39.799675	-2.012242	2.461773	0.007565	0.701745
-39.911200	-1.993000	2.471770	0.007586	0.701744
-39.685762	-1.955565	2.481766	0.007544	0.701901
-39.000594	-1.992114	2.491763	0.007417	0.702074
-38.865107	-2.015712	2.501760	0.007392	0.702074
-39.113588	-1.955677	2.511757	0.007438	0.702106
-38.415822	-1.949002	2.521754	0.007308	0.702371
-38.033664	-2.017540	2.531750	0.007237	0.702370
-38.115836	-2.000171	2.541747	0.007253	0.702375
-37.666466	-1.961839	2.551744	0.007169	0.702614
-37.537612	-1.942771	2.561741	0.007145	0.702699
-37.225978	-1.997266	2.571738	0.007087	0.702701
-37.137136	-1.951416	2.581734	0.007071	0.702825
-36.360552	-1.999533	2.591731	0.006927	0.703007
-36.544119	-1.964550	2.601728	0.006961	0.703012
-36.554887	-1.952984	2.611725	0.006963	0.703031
-35.771270	-1.939095	2.621722	0.006817	0.703341
-35.490479	-1.991573	2.631718	0.006765	0.703336
-35.555601	-1.979717	2.641715	0.006777	0.703336
-34.970621	-1.997901	2.651712	0.006669	0.703510
-34.694172	-1.985457	2.661709	0.006617	0.703634
-34.579279	-2.005109	2.671706	0.006596	0.703635
-34.602169	-2.000123	2.681702	0.006600	0.703637
-33.949056	-1.965654	2.691699	0.006479	0.703941
-33.514921	-2.034581	2.701696	0.006398	0.703958
-33.785570	-1.986206	2.711693	0.006449	0.703958
-33.577435	-1.966384	2.721690	0.006410	0.704072
-32.819524	-2.007273	2.731686	0.006269	0.704262
-32.763107	-2.017895	2.741683	0.006259	0.704261
-32.740399	-2.020378	2.751680	0.006255	0.704264
-32.190201	-1.998937	2.761677	0.006152	0.704504
-31.954847	-1.996948	2.771674	0.006109	0.704593
-32.099503	-1.972040	2.781670	0.006136	0.704591
-31.882793	-1.974205	2.791667	0.006096	0.704664
-30.954650	-2.027195	2.801664	0.005923	0.704890
-30.915628	-2.032157	2.811661	0.005916	0.704894
-30.886965	-2.036902	2.821658	0.005911	0.704894
-30.648859	-1.983736	2.831654	0.005866	0.705087
-29.954031	-2.045558	2.841651	0.005737	0.705211
-30.082360	-2.021195	2.851648	0.005761	0.705214
-30.111878	-2.015027	2.861645	0.005767	0.705216
-29.623973	-1.954277	2.871642	0.005676	0.705513
-29.387414	-1.989515	2.881638	0.005632	0.705527
-29.181591	-2.025835	2.891635	0.005594	0.705527
-28.975850	-1.970654	2.901632	0.005556	0.705712
-28.302730	-2.013433	2.911629	0.005431	0.705867
-28.240930	-2.025482	2.921626	0.005419	0.705864
-28.471784	-1.985410	2.931622	0.005462	0.705862
-27.740432	-1.983371	2.941619	0.005326	0.706128
-27.654261	-1.998015	2.951616	0.005310	0.706129
-27.577520	-2.009540	2.961613	0.005296	0.706133
-27.210837	-1.970987	2.971610	0.005228	0.706342
-26.837930	-1.985884	2.981606	0.005159	0.706445
-26.733865	-2.003366	2.991603	0.005140	0.706447
-26.636845	-1.973324	3.001600	0.005122	0.706542
-25.559749	-2.057814	3.011597	0.004921	0.706758
-25.636634	-2.044447	3.021594	0.004936	0.706757
-25.940007	-1.993206	3.031590	0.004992	0.706751
-25.360735	-1.988978	3.041587	0.004885	0.706966
-24.878383	-2.016791	3.051584	0.004795	0.707083
-24.884688	-2.013824	3.061581	0.004796	0.707086
-24.916783	-1.988982	3.071578	0.004802	0.707124
-24.224484	-1.986965	3.081574	0.004674	0.707376
-23.931730	-2.037799	3.091571	0.004619	0.707378
-24.023138	-2.020716	3.101568	0.004636	0.707380
-23.594519	-1.993236	3.111565	0.004557	0.707588
-23.448348	-1.962056	3.121562	0.004530	0.707702
-23.317959	-1.986875	3.131558	0.004505	0.707699
-23.084465	-1.984882	3.141555	0.004462	0.707786
-22.312049	-2.008588	3.151552	0.004318	0.708015
-22.129956	-2.041179	3.161549	0.004285	0.708014
-22.516476	-1.972481	3.171546	0.004357	0.708013
-21.715703	-1.976562	3.181542	0.004208	0.708291
-21.429743	-2.000605	3.191539	0.004155	0.708345
-21.280519	-2.024687	3.201536	0.004127	0.708349
-21.126787	-2.031910	3.211533	0.004099	0.708390
-20.705140	-1.982354	3.221530	0.004020	0.708639
-20.439305	-2.031115	3.231526	0.003971	0.708636
-20.577241	-2.003791	3.241523	0.003997	0.708641
-20.152651	-1.973597	3.251520	0.003918	0.708853
-19.544574	-2.028401	3.261517	0.003805	0.708960
-19.698251	-2.002525	3.271514	0.003833	0.708957
-19.610685	-1.995753	3.281510	0.003817	0.709001
-18.878343	-1.995353	3.291507	0.003681	0.709263
-18.620231	-2.039106	3.301504	0.003633	0.709268
-18.739060	-2.017606	3.311501	0.003655	0.709268
-18.310903	-1.988259	3.321498	0.003576	0.709479
-17.828863	-2.015004	3.331494	0.003486	0.709597
-17.993169	-1.985792	3.341491	0.003517	0.709597
-17.826777	-1.997497	3.351488	0.003486	0.709632
-16.920522	-2.026863	3.361485	0.003317	0.709896
-16.999140	-2.012372	3.371482	0.003332	0.709897
-16.864727	-2.038223	3.381478	0.003307	0.709893
-16.810049	-1.972601	3.391475	0.003297	0.710043
-15.788406	-2.065842	3.401472	0.003107	0.710221
-16.337447	-1.965970	3.411469	0.003210	0.710225
-16.178816	-1.991835	3.421466	0.003180	0.710229
-15.367386	-1.983766	3.431462	0.003029	0.710534
-15.317649	-1.993122	3.441459	0.003020	0.710533
-15.074361	-2.034070	3.451456	0.002975	0.710537
-15.029928	-1.948201	3.461453	0.002967	0.710724
-14.163015	-2.027122	3.471450	0.002805	0.710875
-14.245445	-2.011053	3.481446	0.002821	0.710877
-14.283904	-2.005830	3.491443	0.002828	0.710874
-13.770477	-1.976619	3.501440	0.002733	0.711115
-13.561652	-1.999599	3.511437	0.002694	0.711143
-13.683471	-1.978156	3.521434	0.002717	0.711142
-13.217443	-1.964340	3.531430	0.002630	0.711335
-12.998487	-1.942905	3.541427	0.002590	0.711455
-12.552784	-2.021319	3.551424	0.002507	0.711457
-12.342031	-2.026185	3.561421	0.002468	0.711522
-11.568826	-2.041724	3.571418	0.002324	0.711765
-11.403109	-2.073820	3.581414	0.002293	0.711760
-11.608418	-2.035819	3.591411	0.002331	0.711763
-11.340119	-2.039674	3.601408	0.002282	0.711850
-10.206310	-2.117981	3.611405	0.002071	0.712096
-10.401661	-2.084891	3.621402	0.002107	0.712093
-10.638350	-2.043260	3.631398	0.002151	0.712091
-10.526161	-2.026182	3.641395	0.002131	0.712165
-9.605989	-2.074645	3.651392	0.001959	0.712395
-9.494998	-2.095542	3.661389	0.001939	0.712392
-9.520892	-2.092249	3.671386	0.001944	0.712389
-9.254984	-2.066841	3.681382	0.001895	0.712534
-8.440823	-2.122723	3.691379	0.001743	0.712711
-8.534129	-2.105342	3.701376	0.001761	0.712713
-8.569477	-2.098129	3.711373	0.001767	0.712714
-8.151476	-2.089692	3.721370	0.001690	0.712879
-7.612438	-2.112414	3.731366	0.001589	0.713025
-7.474951	-2.136618	3.741363	0.001564	0.713025
-7.590878	-2.115914	3.751360	0.001586	0.713025
-7.048117	-2.108810	3.761357	0.001485	0.713231
-6.647267	-2.112335	3.771354	0.001410	0.713366
-6.753469	-2.095328	3.781350	0.001430	0.713362
-6.691294	-2.105566	3.791347	0.001419	0.713363
-5.838587	-2.137509	3.801344	0.001260	0.713602
-5.936129	-2.090179	3.811341	0.001278	0.713661
-5.868555	-2.101338	3.821338	0.001266	0.713663
-6.021022	-2.038876	3.831334	0.001294	0.713732
-5.075472	-2.085481	3.841331	0.001118	0.713974
-5.107684	-2.076900	3.851328	0.001125	0.713980
-5.301844	-2.041043	3.861325	0.001161	0.713982
-4.374926	-2.060094	3.871322	0.000988	0.714272
-4.220906	-2.081577	3.881318	0.000960	0.714284
-3.860603	-2.148771	3.891315	0.000893	0.714277
-3.957938	-2.081072	3.901312	0.000911	0.714377
-3.201321	-2.098741	3.911309	0.000770	0.714610
-2.945505	-2.143586	3.921306	0.000723	0.714611
-3.283664	-2.085504	3.931302	0.000786	0.714606
-2.796665	-2.080733	3.941299	0.000696	0.714788
-2.349948	-2.098407	3.951296	0.000613	0.714910
-2.281219	-2.110714	3.961293	0.000600	0.714910
-2.184547	-2.119929	3.971290	0.000582	0.714925
-2.004004	-1.996452	3.981286	0.000548	0.715234
-1.752095	-2.041189	3.991283	0.000502	0.715234
-1.850556	-2.023127	4.001280	0.000520	0.715235
-1.651551	-1.901215	4.011277	0.000483	0.715547
-1.433378	-1.938406	4.021274	0.000443	0.715550
-1.577010	-1.854409	4.031270	0.000470	0.715665
-1.052703	-1.835440	4.041267	0.000372	0.715888
-1.011059	-1.840479	4.051264	0.000364	0.715892
-0.980373	-1.736318	4.061261	0.000359	0.716109
-1.213047	-1.677829	4.071258	0.000402	0.716143
-1.029113	-1.588615	4.081254	0.000368	0.716384
-0.843080	-1.589186	4.091251	0.000334	0.716449
-0.956796	-1.437278	4.101248	0.000355	0.716709
-0.804374	-1.420558	4.111245	0.000326	0.716796
-0.640175	-1.302799	4.121242	0.000296	0.717086
-0.553085	-1.253566	4.131238	0.000280	0.717214
-0.607538	-1.159561	4.141235	0.000290	0.717381
-0.591403	-1.019738	4.151232	0.000287	0.717663
-0.566230	-0.934642	4.161229	0.000283	0.717840
-0.414545	-0.861970	4.171226	0.000254	0.718036
-0.487168	-0.689596	4.181222	0.000268	0.718351
-0.230873	-0.626378	4.191219	0.000220	0.718566
-0.359298	-0.488050	4.201216	0.000244	0.718794
-0.258611	-0.376425	4.211213	0.000226	0.719049
-0.039719	-0.290475	4.221210	0.000185	0.719295
-0.071360	-0.130707	4.231206	0.000191	0.719599
-0.023763	0.001578	4.241203	0.000182	0.719876
0.000000	0.157780	4.251200	0.000178	0.720192

0.041213	0.768240	4.256205	0.000170	0.721408
0.131417	2.019029	4.261210	0.000152	0.723896
0.631273	3.784588	4.266214	0.000058	0.727522
0.789129	6.172324	4.271219	0.000027	0.732219
1.212008	9.022243	4.276224	-0.000054	0.737866
1.280360	12.401143	4.281229	-0.000068	0.744359
1.739485	16.179129	4.286234	-0.000156	0.751681
2.159171	20.358749	4.291238	-0.000237	0.759669
2.558772	24.941783	4.296243	-0.000314	0.768313
3.148922	29.868269	4.301248	-0.000427	0.777550
3.522860	35.166803	4.306253	-0.000500	0.787279
3.984843	40.784505	4.311258	-0.000590	0.797485
4.421000	46.697894	4.316262	-0.000675	0.808074
4.853497	52.898630	4.321267	-0.000760	0.819022
5.416277	59.351161	4.326272	-0.000868	0.830295
7.338046	65.790823	4.331277	-0.001230	0.841799
8.380011	72.637797	4.336282	-0.001429	0.853567
8.976475	79.765066	4.341286	-0.001544	0.865505
9.419258	87.103357	4.346291	-0.001632	0.877577
10.139651	94.576577	4.351296	-0.001771	0.889779
11.652105	102.065757	4.356301	-0.002057	0.902058
12.623640	109.819336	4.361306	-0.002243	0.914435
13.212180	117.740714	4.366310	-0.002358	0.926801
14.221480	125.721568	4.371315	-0.002551	0.939204
14.789253	133.885553	4.376320	-0.002662	0.951603
15.732295	142.056160	4.381325	-0.002842	0.963948
16.847790	150.304644	4.386330	-0.003055	0.976293
17.822292	158.656816	4.391334	-0.003242	0.988597
18.339434	167.136142	4.396339	-0.003344	1.000816
18.931318	175.637639	4.401344	-0.003460	1.012938
20.324203	184.050028	4.406349	-0.003724	1.024984
20.952852	192.646290	4.411354	-0.003847	1.036960
21.403418	201.279942	4.416358	-0.003937	1.048808
21.862936	209.936396	4.421363	-0.004028	1.060555
23.158148	218.484299	4.426368	-0.004274	1.072221
23.832939	227.122445	4.431373	-0.004406	1.083739
24.629773	235.759516	4.436378	-0.004559	1.095161
25.493288	244.377895	4.441382	-0.004726	1.106456
26.201455	253.036956	4.446387	-0.004863	1.117653
26.887954	261.702981	4.451392	-0.004997	1.128744
27.540259	270.365170	4.456397	-0.005124	1.139713
28.539310	278.992175	4.461402	-0.005315	1.150608
28.889044	287.698038	4.466406	-0.005386	1.161361
29.332357	296.356663	4.471411	-0.005474	1.171977
30.180409	304.940293	4.476416	-0.005638	1.182490
30.749852	313.557370	4.481421	-0.005749	1.192894
31.438304	322.142636	4.486426	-0.005883	1.203194
32.301363	330.690066	4.491430	-0.006049	1.213396
32.860033	339.275104	4.496435	-0.006159	1.223497
33.479620	347.878970	4.501440	-0.006279	1.233548
34.208616	356.392708	4.506445	-0.006421	1.243436
34.991134	364.918933	4.511450	-0.006572	1.253270
35.689977	373.430214	4.516454	-0.006708	1.262994
36.416685	381.937870	4.521459	-0.006848	1.272645
37.211662	390.413921	4.526464	-0.007002	1.282201
37.609674	398.938079	4.531469	-0.007081	1.291665
38.258070	407.411901	4.536474	-0.007208	1.301051
38.905191	415.927802	4.541478	-0.007334	1.310415
39.370302	424.463605	4.546483	-0.007426	1.319700
40.208089	432.838927	4.551488	-0.007587	1.328816
41.090771	441.209668	4.556493	-0.007757	1.337873
41.589892	449.635496	4.561498	-0.007855	1.346859
41.991316	458.074551	4.566502	-0.007935	1.355781
42.563249	466.452739	4.571507	-0.008047	1.364612
43.233821	474.837714	4.576512	-0.008177	1.373409
43.588742	483.230474	4.581517	-0.008249	1.382105
44.129385	491.615897	4.586522	-0.008355	1.390770
44.549214	499.994867	4.591526	-0.008439	1.399354
45.113536	508.313249	4.596531	-0.008549	1.407848
45.485091	516.699986	4.601536	-0.008624	1.416328
46.009510	525.012588	4.606541	-0.008727	1.424709
46.587492	533.356982	4.611546	-0.008840	1.433081
46.971532	541.677764	4.616550	-0.008916	1.441349
47.251284	550.024189	4.621555	-0.008974	1.449578
47.791389	558.344437	4.626560	-0.009080	1.457777
48.118046	566.642422	4.631565	-0.009146	1.465874
48.486898	575.012691	4.636570	-0.009220	1.474003
49.195458	583.238492	4.641574	-0.009357	1.482002
49.941196	591.457054	4.646579	-0.009501	1.489956
50.536395	599.733610	4.651584	-0.009618	1.497900
50.764747	608.022715	4.656589	-0.009665	1.505757
51.563550	616.256243	4.661594	-0.009819	1.513609
51.761856	624.555703	4.666598	-0.009862	1.521389
52.206358	632.813846	4.671603	-0.009950	1.529129
52.918518	641.056127	4.676608	-0.010088	1.536855
52.987481	649.336519	4.681613	-0.010106	1.544482
53.543455	657.600713	4.686618	-0.010215	1.552128
54.102972	665.815627	4.691622	-0.010324	1.559693
54.746449	674.011332	4.696627	-0.010449	1.567215
55.275496	682.254592	4.701632	-0.010553	1.574728
55.610724	690.479182	4.706637	-0.010621	1.582160
56.226069	698.683833	4.711642	-0.010741	1.589579
56.680802	706.924190	4.716646	-0.010831	1.596972
56.961637	715.155929	4.721651	-0.010888	1.604299
57.489710	723.377009	4.726656	-0.010992	1.611619
57.667058	731.627684	4.731661	-0.011030	1.618881
58.201693	739.819148	4.736666	-0.011135	1.626109
58.668955	748.077182	4.741670	-0.011227	1.633354
59.176080	756.246631	4.746675	-0.011327	1.640495
59.565368	764.449996	4.751680	-0.011405	1.647618
60.058375	772.630914	4.756685	-0.011502	1.654705
60.691425	780.785521	4.761690	-0.011625	1.661759
61.360719	788.957439	4.766694	-0.011755	1.668802
61.755831	797.167650	4.771699	-0.011834	1.675811
62.465271	805.307716	4.776704	-0.011971	1.682773
62.619157	813.519445	4.781709	-0.012005	1.689693
63.215624	821.699306	4.786714	-0.012121	1.696616
63.801918	829.854602	4.791718	-0.012236	1.703489
64.273235	838.042368	4.796723	-0.012329	1.710346
64.787530	846.237657	4.801728	-0.012430	1.717187
64.986832	854.420871	4.806733	-0.012472	1.723951
65.344581	862.606089	4.811738	-0.012544	1.730710
65.671293	870.802151	4.816742	-0.012610	1.737447
65.964996	878.959645	4.821747	-0.012670	1.744123
66.465734	887.134327	4.826752	-0.012768	1.750813
66.865169	895.290196	4.831757	-0.012848	1.757450
67.294532	903.438842	4.836762	-0.012933	1.764060
67.545534	911.629097	4.841766	-0.012985	1.770656
68.090687	919.760981	4.846771	-0.013092	1.777217
68.439990	927.916536	4.851776	-0.013162	1.783748
68.767380	936.091946	4.856781	-0.013229	1.790269
69.145590	944.285488	4.861786	-0.013304	1.796786
69.571001	952.401129	4.866790	-0.013389	1.803224
69.555486	960.584587	4.871795	-0.013391	1.809639
69.953915	968.729459	4.876800	-0.013470	1.816051
70.189706	976.866517	4.881805	-0.013520	1.822415
70.677074	984.990348	4.886810	-0.013616	1.828776
71.204675	993.123626	4.891814	-0.013719	1.835127
71.577874	1001.235218	4.896819	-0.013794	1.841422
72.163453	1009.357059	4.901824	-0.013908	1.847727
72.249051	1017.540203	4.906829	-0.013929	1.853999
72.840400	1025.649067	4.911834	-0.014045	1.860252
73.191262	1033.795131	4.916838	-0.014115	1.866485
73.639952	1041.934458	4.921843	-0.014204	1.872702
74.086920	1050.077513	4.926848	-0.014292	1.878902
74.359510	1058.176339	4.931853	-0.014348	1.885028
75.084026	1066.264224	4.936858	-0.014488	1.891177
75.709238	1074.365099	4.941862	-0.014610	1.897305
75.746115	1082.538409	4.946867	-0.014622	1.903400
76.085472	1090.693076	4.951872	-0.014691	1.909496
76.402171	1098.815052	4.956877	-0.014755	1.915546
76.768766	1106.940232	4.961882	-0.014828	1.921584
77.190696	1115.039849	4.966886	-0.014912	1.927591
77.496154	1123.175184	4.971891	-0.014974	1.933592
77.941687	1131.286604	4.976896	-0.015062	1.939573
78.100324	1139.416331	4.981901	-0.015097	1.945517
78.640642	1147.557774	4.986906	-0.015203	1.951492
78.880479	1155.704677	4.991910	-0.015253	1.957421
79.067488	1163.804545	4.996915	-0.015293	1.963293
79.483665	1171.899196	5.001920	-0.015376	1.969167
79.681927	1180.023224	5.006925	-0.015418	1.975022
80.116868	1188.104873	5.011930	-0.015504	1.980854
80.587167	1196.200873	5.016934	-0.015597	1.986683
81.013442	1204.301681	5.021939	-0.015681	1.992493
81.267054	1212.433166	5.026944	-0.015734	1.998290
81.660473	1220.505052	5.031949	-0.015812	2.004043
81.716619	1228.661645	5.036954	-0.015828	2.009804
81.913183	1236.800976	5.041958	-0.015870	2.015551
82.317328	1244.858462	5.046963	-0.015950	2.021245
82.807276	1252.946718	5.051968	-0.016047	2.026954
83.072493	1261.082505	5.056973	-0.016101	2.032656
83.424903	1269.190366	5.061978	-0.016172	2.038332
83.805090	1277.257117	5.066982	-0.016248	2.043966
84.154503	1285.354799	5.071987	-0.016318	2.049604
84.661001	1293.456403	5.076992	-0.016418	2.055244
84.967824	1301.538735	5.081997	-0.016480	2.060835
85.490749	1309.617908	5.087002	-0.016583	2.066430
85.906740	1317.737732	5.092006	-0.016665	2.072028
86.166881	1325.833812	5.097011	-0.016719	2.077578
86.493677	1333.932207	5.102016	-0.016785	2.083122
86.866147	1342.010360	5.107021	-0.016860	2.088641
87.052649	1350.156067	5.112026	-0.016900	2.094174
87.450548	1358.231545	5.117030	-0.016979	2.099665
87.528387	1366.346878	5.122035	-0.016999	2.105137
88.176162	1374.423515	5.127040	-0.017124	2.110625
88.573749	1382.547005	5.132045	-0.017204	2.116105
89.011083	1390.603581	5.137050	-0.017290	2.121530
89.117163	1398.709733	5.142054	-0.017315	2.126943
89.214321	1406.831326	5.147059	-0.017339	2.132351
89.521494	1414.914778	5.152064	-0.017401	2.137740
89.739512	1422.985553	5.157069	-0.017447	2.143098
90.044459	1431.061207	5.162074	-0.017509	2.148455
90.701573	1439.128619	5.167078	-0.017636	2.153826
91.158003	1447.182421	5.172083	-0.017726	2.159155
91.643885	1455.253482	5.177088	-0.017822	2.164486
92.060307	1463.338178	5.182093	-0.017905	2.169805
92.289044	1471.471355	5.187098	-0.017953	2.175126
92.488840	1479.561408	5.192102	-0.017995	2.180403
92.886396	1487.615038	5.197107	-0.018074	2.185662
93.471452	1495.701017	5.202112	-0.018188	2.190946
93.829954	1503.801151	5.207117	-0.018260	2.196205
94.542085	1511.804873	5.212122	-0.018398	2.201422
95.310596	1519.851332	5.217126	-0.018546	2.206659
95.828512	1527.941232	5.222131	-0.018648	2.211889
96.161822	1536.060681	5.227136	-0.018715	2.217108
96.119036	1544.185556	5.232141	-0.018713	2.222285
96.616251	1552.237343	5.237146	-0.018810	2.227452
96.956495	1560.359432	5.242150	-0.018879	2.232637
97.265039	1568.434746	5.247155	-0.018942	2.237778
97.885313	1576.486669	5.252160	-0.019062	2.242919
98.108413	1584.576337	5.257165	-0.019109	2.248038
98.193517	1592.711740	5.262170	-0.019130	2.253161
98.656027	1600.772529	5.267174	-0.019221	2.258259
98.742235	1608.852581	5.272179	-0.019243	2.263325
99.126609	1616.933830	5.277184	-0.019319	2.268406
99.438402	1625.081875	5.282189	-0.019383	2.273511
99.617658	1633.138327	5.287194	-0.019421	2.278536
100.017468	1641.165445	5.292198	-0.019501	2.283550
100.080588	1649.247724	5.297203	-0.019518	2.288559
100.590878	1657.291407	5.302208	-0.019618	2.293571
101.023384	1665.333550	5.307213	-0.019704	2.298565
101.309486	1673.400333	5.312218	-0.019762	2.303550
101.628077	1681.471955	5.317222	-0.019827	2.308530
101.916241	1689.563354	5.322227	-0.019886	2.313509
102.229297	1697.638824	5.327232	-0.019949	2.318470
102.334182	1705.711981	5.332237	-0.019974	2.323401
102.759329	1713.766533	5.337242	-0.020058	2.328337
103.272155	1721.826575	5.342246	-0.020159	2.333273
103.433804	1729.902136	5.347251	-0.020194	2.338179
103.863771	1737.962333	5.352256	-0.020279	2.343087
104.225069	1746.015864	5.357261	-0.020352	2.347975
104.466412	1754.153499	5.362266	-0.020402	2.352894
104.854718	1762.207902	5.367270	-0.020479	2.357765
105.219836	1770.238568	5.372275	-0.020553	2.362609
105.568820	1778.316869	5.377280	-0.020623	2.367470
105.783195	1786.384285	5.382285	-0.020668	2.372305
106.222464	1794.438440	5.387290	-0.020755	2.377139
106.555211	1802.484920	5.392294	-0.020822	2.381950
106.633948	1810.577623	5.397299	-0.020842	2.386759
107.205927	1818.630939	5.402304	-0.020953	2.391574
107.446489	1826.703514	5.407309	-0.021003	2.396364
107.578670	1834.779543	5.412314	-0.021033	2.401138
108.234021	1842.808103	5.417318	-0.021160	2.405916
108.782923	1850.841649	5.422323	-0.021268	2.410678
109.119594	1858.949669	5.427328	-0.021336	2.415459
109.049667	1867.039092	5.432333	-0.021328	2.420187
109.276080	1875.110261	5.437338	-0.021375	2.424918
109.755174	1883.163509	5.442342	-0.021470	2.429650
109.794023	1891.335039	5.447347	-0.021482	2.434406
110.171628	1899.360738	5.452352	-0.021558	2.439095
110.429933	1907.377346	5.457357	-0.021611	2.443760
110.415708	1915.457856	5.462362	-0.021613	2.448433
110.553666	1923.554192	5.467366	-0.021644	2.453118
111.035786	1931.543860	5.472371	-0.021739	2.457758
111.676635	1939.553780	5.477376	-0.021864	2.462412
111.655025	1947.642963	5.482381	-0.021865	2.467054
111.853549	1955.733203	5.487386	-0.021907	2.471704
112.502225	1963.739381	5.492390	-0.022033	2.476330
112.893395	1971.755742	5.497395	-0.022111	2.480935
113.073121	1979.857410	5.502400	-0.022150	2.485563
113.421099	1987.895681	5.507405	-0.022220	2.490160
113.929008	1995.960877	5.512410	-0.022319	2.494775
114.145736	2004.037217	5.517414	-0.022365	2.499366
114.408529	2012.083118	5.522419	-0.022419	2.503935
114.774154	2020.146735	5.527424	-0.022492	2.508513
114.646592	2028.297455	5.532429	-0.022474	2.513097
115.208217	2036.292767	5.537434	-0.022583	2.517634
115.622596	2044.334215	5.542438	-0.022666	2.522178
116.012816	2052.358108	5.547443	-0.022744	2.526702
116.129819	2060.466659	5.552448	-0.022771	2.531246
116.463699	2068.513290	5.557453	-0.022838	2.535762
116.707735	2076.562635	5.562458	-0.022889	2.540266
116.778984	2084.621953	5.567462	-0.022907	2.544755
117.125991	2092.677499	5.572467	-0.022977	2.549253
117.395116	2100.764957	5.577472	-0.023032	2.553756
117.534034	2108.804262	5.582477	-0.023063	2.558215
117.893818	2116.846805	5.587482	-0.023135	2.562683
118.143242	2124.896828	5.592486	-0.023187	2.567140
118.366918	2132.949199	5.597491	-0.023234	2.571588
118.741596	2140.999266	5.602496	-0.023309	2.576038
119.134161	2149.017678	5.607501	-0.023387	2.580464
119.540004	2157.052153	5.612506	-0.023468	2.584893
119.876444	2165.143908	5.617510	-0.023536	2.589339
120.188270	2173.366789	5.622515	-0.023599	2.593849
120.348158	2181.406600	5.627520	-0.023634	2.598240
120.580922	2189.380973	5.632525	-0.023682	2.602593
121.067008	2197.375092	5.637530	-0.023778	2.606967
121.294744	2205.446368	5.642534	-0.023826	2.611357
121.534594	2213.503605	5.647539	-0.023875	2.615734
121.805380	2221.539437	5.652544	-0.023931	2.620093
121.990691	2229.576193	5.657549	-0.023971	2.624440
122.390620	2237.612442	5.662554	-0.024050	2.628794
122.809615	2245.680552	5.667558	-0.024134	2.633159
123.001158	2253.733172	5.672563	-0.024174	2.637493
123.309730	2261.766740	5.677568	-0.024237	2.641818
123.603028	2269.796549	5.682573	-0.024297	2.646132
123.805948	2277.854782	5.687578	-0.024340	2.650449
124.047312	2285.932141	5.692582	-0.024390	2.654771
124.215953	2293.967395	5.697587	-0.024426	2.659059
124.773835	2301.987811	5.702592	-0.024536	2.663358
124.968603	2310.032026	5.707597	-0.024577	2.667638
125.275111	2318.108776	5.712602	-0.024639	2.671936
125.616517	2326.181502	5.717606	-0.024708	2.676227
125.632756	2334.218496	5.722611	-0.024716	2.680472
126.126925	2342.215954	5.727616	-0.024813	2.684720
126.384238	2350.272695	5.732621	-0.024866	2.688976
126.590839	2358.341917	5.737626	-0.024910	2.693230
127.043129	2366.380849	5.742630	-0.024999	2.697476
127.117712	2374.414144	5.747635	-0.025019	2.701689
127.506528	2382.463072	5.752640	-0.025096	2.705923
127.724682	2390.506327	5.757645	-0.025142	2.710137
128.007178	2398.579734	5.762650	-0.025200	2.714364
128.391300	2406.607589	5.767654	-0.025276	2.718567
128.679221	2414.631874	5.772659	-0.025335	2.722755
128.981634	2422.692257	5.777664	-0.025397	2.726957
129.222924	2430.745961	5.782669	-0.025447	2.731144
129.305313	2438.846659	5.787674	-0.025467	2.735340
129.712682	2446.849523	5.792678	-0.025548	2.739499
129.962703	2454.852434	5.797683	-0.025600	2.743642
130.244251	2462.934865	5.802688	-0.025658	2.747822
130.622478	2471.007482	5.807693	-0.025733	2.751995
131.161670	2479.060931	5.812698	-0.025839	2.756163
131.437669	2487.085771	5.817702	-0.025895	2.760293
131.578402	2495.111742	5.822707	-0.025927	2.764410
131.924525	2503.153927	5.827712	-0.025996	2.768541
131.917569	2511.234749	5.832717	-0.026000	2.772664
132.146016	2519.275103	5.837722	-0.026048	2.776775
132.516169	2527.300625	5.842726	-0.026122	2.780880
132.780663	2535.315414	5.847731	-0.026176	2.784968
133.003527	2543.397449	5.852736	-0.026223	2.789081
133.227077	2551.437195	5.857741	-0.026270	2.793167
133.328694	2559.482517	5.862746	-0.026294	2.797243
133.565694	2567.511689	5.867750	-0.026343	2.801312
133.899258	2575.511850	5.872755	-0.026411	2.805366
134.532669	2583.555154	5.877760	-0.026534	2.809453
134.766376	2591.619634	5.882765	-0.026582	2.813522
134.906956	2599.681683	5.887770	-0.026614	2.817579
135.165404	2607.732021	5.892774	-0.026667	2.821630
135.517392	2615.741623	5.897779	-0.026738	2.825661
135.717424	2623.816381	5.902784	-0.026780	2.829709
135.983492	2631.879059	5.907789	-0.026835	2.833750
136.096296	2639.913112	5.912794	-0.026861	2.837761
136.674376	2647.941126	5.917798	-0.026974	2.841791
136.588685	2655.975988	5.922803	-0.026963	2.845780
137.054054	2663.994593	5.927808	-0.027055	2.849787
137.183161	2672.048714	5.932813	-0.027084	2.853787
137.452224	2680.090292	5.937818	-0.027139	2.857783
137.634216	2688.139770	5.942822	-0.027178	2.861772
138.006282	2696.142610	5.947827	-0.027253	2.865743
138.249438	2704.194613	5.952832	-0.027303	2.869726
138.339358	2712.284551	5.957837	-0.027325	2.873714
138.675101	2720.275799	5.962842	-0.027393	2.877660
139.053808	2728.331347	5.967846	-0.027469	2.881636
139.150364	2736.347961	5.972851	-0.027492	2.885571
139.545791	2744.398002	5.977856	-0.027571	2.889533
139.841061	2752.440993	5.982861	-0.027631	2.893481
139.990903	2760.499025	5.987866	-0.027664	2.897424
140.160459	2768.542241	5.992870	-0.027701	2.901354
140.632596	2776.547155	5.997875	-0.027794	2.905277
141.061907	2784.601906	6.002880	-0.027879	2.909216
141.312378	2792.723437	6.007885	-0.027931	2.913173
141.735391	2800.740002	6.012890	-0.028015	2.917083
141.816938	2808.774508	6.017894	-0.028035	2.920978
141.919514	2816.751607	6.022899	-0.028059	2.924841
142.280603	2824.806932	6.027904	-0.028132	2.928750
142.453417	2832.839901	6.032909	-0.028169	2.932634
142.629069	2840.907958	6.037914	-0.028207	2.936529
142.800354	2848.943788	6.042918	-0.028244	2.940404
142.990669	2856.935587	6.047923	-0.028284	2.944253
143.312167	2864.999999	6.052928	-0.028349	2.948138
143.438181	2873.024539	6.057933	-0.028378	2.951990
143.776561	2881.074694	6.062938	-0.028446	2.955859
144.139344	2889.095054	6.067942	-0.028519	2.959710
144.383494	2897.098824	6.072947	-0.028570	2.963543
144.661420	2905.171751	6.077952	-0.028627	2.967405
144.941127	2913.215126	6.082957	-0.028684	2.971247
145.104450	2921.276197	6.087962	-0.028719	2.975088
145.517791	2929.287009	6.092966	-0.028801	2.978912
145.713031	2937.312354	6.097971	-0.028843	2.982727
146.000291	2945.364736	6.102976	-0.028902	2.986555
146.180806	2953.409157	6.107981	-0.028940	2.990368
146.336097	2961.482481	6.112986	-0.028975	2.994189
146.851424	2969.479320	6.117990	-0.029076	2.997987
146.751420	2977.524015	6.122995	-0.029062	3.001772
146.984327	2985.562510	6.128000	-0.029111	3.005566
147.388655	2993.562111	6.133005	-0.029191	3.009345
147.813095	3001.616481	6.138010	-0.029275	3.013146
148.086535	3009.653671	6.143014	-0.029331	3.016927
148.104362	3017.682313	6.148019	-0.029340	3.020686
148.387049	3025.727543	6.153024	-0.029398	3.024462
148.584086	3033.759748	6.158029	-0.029440	3.028222
148.678772	3041.824022	6.163034	-0.029462	3.031988
149.006628	3049.868268	6.168038	-0.029529	3.035751
149.286660	3057.840982	6.173043	-0.029586	3.039474
149.513332	3065.886929	6.178048	-0.029633	3.043223
149.887501	3073.902876	6.183053	-0.029708	3.046961
150.284908	3081.941313	6.188058	-0.029787	3.050706
150.296564	3090.041439	6.193062	-0.029795	3.054457
150.304006	3098.050621	6.198067	-0.029801	3.058160
150.592979	3106.084810	6.203072	-0.029860	3.061884
150.636316	3114.119373	6.208077	-0.029873	3.065592
150.875366	3122.143152	6.213082	-0.029923	3.069300
151.257130	3130.245816	6.218086	-0.029999	3.073046
151.583755	3138.271021	6.223091	-0.030065	3.076749
151.850950	3146.273955	6.228096	-0.030120	3.080435
151.990578	3154.274934	6.233101	-0.030151	3.084110
152.375301	3162.288190	6.238106	-0.030228	3.087797
152.581837	3170.364617	6.243110	-0.030272	3.091500
152.630752	3178.422172	6.248115	-0.030286	3.095183
152.873434	3186.433711	6.253120	-0.030336	3.098850
153.075092	3194.463072	6.258125	-0.030379	3.102518
153.245301	3202.503118	6.263130	-0.030416	3.106185
153.827226	3210.484383	6.268134	-0.030530	3.109840
153.916143	3218.550352	6.273139	-0.030551	3.113507
154.066939	3226.612873	6.278144	-0.030585	3.117171
154.194344	3234.629351	6.283149	-0.030613	3.120808
154.593442	3242.603631	6.288154	-0.030693	3.124434
154.879463	3250.676603	6.293158	-0.030751	3.128096
154.907448	3258.722235	6.298163	-0.030762	3.131729
155.169199	3266.757106	6.303168	-0.030816	3.135364
155.875088	3274.725429	6.308173	-0.030952	3.138984
156.134115	3282.760100	6.313178	-0.031006	3.142610
156.544788	3290.814452	6.318182	-0.031087	3.146247
156.525357	3298.855399	6.323187	-0.031089	3.149855
156.940033	3306.926184	6.328192	-0.031171	3.153491
157.333496	3314.961116	6.333197	-0.031250	3.157106
157.448139	3322.959754	6.338202	-0.031276	3.160689
157.719508	3330.960117	6.343206	-0.031332	3.164275
157.788210	3339.008091	6.348211	-0.031350	3.167869
158.214104	3347.066005	6.353216	-0.031434	3.171479
158.420404	3355.101734	6.358221	-0.031478	3.175065
158.433993	3363.162269	6.363226	-0.031486	3.178651
158.966682	3371.164824	6.368230	-0.031590	3.182228
158.917427	3379.197558	6.373235	-0.031586	3.185790
159.160510	3387.251667	6.378240	-0.031636	3.189370
159.401417	3395.291170	6.383245	-0.031686	3.192940
159.383892	3403.341642	6.388250	-0.031688	3.196499
159.874662	3411.307134	6.393254	-0.031785	3.200038
159.844133	3419.349212	6.398259	-0.031784	3.203586
160.406235	3427.361491	6.403264	-0.031894	3.207140
160.616482	3435.399636	6.408269	-0.031938	3.210688
160.772288	3443.449039	6.413274	-0.031973	3.214234
161.206002	3451.473631	6.418278	-0.032058	3.217777
161.431884	3459.498188	6.423283	-0.032106	3.221307
161.680593	3467.531682	6.428288	-0.032157	3.224839
161.838180	3475.592559	6.433293	-0.032192	3.228374
162.154025	3483.632699	6.438298	-0.032256	3.231903
162.415915	3491.710375	6.443302	-0.032310	3.235443
162.351618	3499.673220	6.448307	-0.032303	3.238915
162.564657	3507.710780	6.453312	-0.032348	3.242427
162.998785	3515.691666	6.458317	-0.032434	3.245920
163.135825	3523.698543	6.463322	-0.032464	3.249408
163.311678	3531.780283	6.468326	-0.032502	3.252927
163.516419	3539.812094	6.473331	-0.032545	3.256421
163.808581	3547.825946	6.478336	-0.032605	3.259907
164.083870	3555.851503	6.483341	-0.032661	3.263393
164.392698	3563.871913	6.488346	-0.032724	3.266875
164.445707	3571.935024	6.493350	-0.032739	3.270362
164.689012	3579.959205	6.498355	-0.032790	3.273836
164.897733	3588.010360	6.503360	-0.032834	3.277316
165.040163	3596.034083	6.508365	-0.032865	3.280778
165.297396	3604.005250	6.513370	-0.032918	3.284218
165.686153	3612.059608	6.518374	-0.032996	3.287695
165.843205	3620.101189	6.523379	-0.033030	3.291154
166.170657	3628.141229	6.528384	-0.033097	3.294616
166.198708	3636.186620	6.533389	-0.033107	3.298064
166.624828	3644.183981	6.538394	-0.033191	3.301504
166.896799	3652.191850	6.543398	-0.033247	3.304938
166.978580	3660.234490	6.548403	-0.033268	3.308377
167.271630	3668.294013	6.553408	-0.033327	3.311827
167.684141	3676.354519	6.558413	-0.033409	3.315278
167.688436	3684.342072	6.563418	-0.033415	3.318680
167.906508	3692.360239	6.568422	-0.033461	3.322099
167.868586	3700.343712	6.573427	-0.033459	3.325490
168.249635	3708.388587	6.578432	-0.033535	3.328919
168.458945	3716.447302	6.583437	-0.033579	3.332344
168.897941	3724.470900	6.588442	-0.033666	3.335759
169.081370	3732.510295	6.593446	-0.033706	3.339168
169.065823	3740.541931	6.598451	-0.033708	3.342563
169.457632	3748.566609	6.603456	-0.033786	3.345966
169.549163	3756.596587	6.608461	-0.033808	3.349358
169.700425	3764.657054	6.613466	-0.033842	3.352760
169.909592	3772.726769	6.618470	-0.033886	3.356165
170.147099	3780.667209	6.623475	-0.033935	3.359514
170.405795	3788.710526	6.628480	-0.033988	3.362903
170.683290	3796.749327	6.633485	-0.034045	3.366287
170.879006	3804.747424	6.638490	-0.034087	3.369648
171.355876	3812.818558	6.643494	-0.034181	3.373046
171.415797	3820.863834	6.648499	-0.034197	3.376415
171.561657	3828.862129	6.653504	-0.034229	3.379764
171.995281	3836.852491	6.658509	-0.034315	3.383116
172.027597	3844.907077	6.663514	-0.034327	3.386478
172.364359	3852.929252	6.668518	-0.034394	3.389833
172.550156	3861.040395	6.673523	-0.034434	3.393217
172.655402	3869.081583	6.678528	-0.034459	3.396566
172.852976	3877.035160	6.683533	-0.034501	3.399878
172.925232	3885.029542	6.688538	-0.034519	3.403200
173.459709	3893.041787	6.693542	-0.034624	3.406541
173.449002	3901.060353	6.698547	-0.034627	3.409863
173.606253	3909.134806	6.703552	-0.034662	3.413211
173.847562	3917.171853	6.708557	-0.034712	3.416543
174.131034	3925.138566	6.713562	-0.034770	3.419844
174.302808	3933.180507	6.718566	-0.034807	3.423169
174.476920	3941.194561	6.723571	-0.034844	3.426479
174.744149	3949.243770	6.728576	-0.034899	3.429803
175.082531	3957.267072	6.733581	-0.034968	3.433116
175.178512	3965.317128	6.738586	-0.034991	3.436429
175.590922	3973.305377	6.743590	-0.035073	3.439724
175.754127	3981.332952	6.748595	-0.035108	3.443023
176.071237	3989.363579	6.753600	-0.035172	3.446326
176.179687	3997.398940	6.758605	-0.035198	3.449620
176.159782	4005.462978	6.763610	-0.035199	3.452919
176.469420	4013.521463	6.768614	-0.035262	3.456223
176.754284	4021.483462	6.773619	-0.035320	3.459483
177.168022	4029.496489	6.778624	-0.035402	3.462766
177.130105	4037.538473	6.783629	-0.035400	3.466042
177.275298	4045.581284	6.788634	-0.035433	3.469322
177.540219	4053.646161	6.793638	-0.035487	3.472611
177.588022	4061.692051	6.798643	-0.035501	3.475883
177.507141	4069.711008	6.803648	-0.035491	3.479136
178.023583	4077.673854	6.808653	-0.035593	3.482383
178.385408	4085.661047	6.813658	-0.035665	3.485631
178.908987	4093.684183	6.818662	-0.035768	3.488896
179.096769	4101.710996	6.823667	-0.035808	3.492149
179.519929	4109.760427	6.828672	-0.035892	3.495415
179.686645	4117.769286	6.833677	-0.035928	3.498654
179.735990	4125.816360	6.838682	-0.035942	3.501902
180.005769	4133.833096	6.843686	-0.035998	3.505141
180.023655	4141.882084	6.848691	-0.036006	3.508382
180.131840	4149.918439	6.853696	-0.036032	3.511618
180.416831	4157.934037	6.858701	-0.036090	3.514848
180.603491	4165.966948	6.863706	-0.036130	3.518079
180.706228	4173.998897	6.868710	-0.036154	3.521304
180.793277	4181.962294	6.873715	-0.036175	3.524498
181.226637	4190.012958	6.878720	-0.036261	3.527735
181.448083	4198.055136	6.883725	-0.036308	3.530958
181.714212	4206.055314	6.888730	-0.036362	3.534164
181.999679	4214.129493	6.893734	-0.036421	3.537396
182.263497	4222.120424	6.898739	-0.036475	3.540592
182.277626	4230.142753	6.903744	-0.036483	3.543790
182.433181	4238.200288	6.908749	-0.036517	3.547003
182.657443	4246.220087	6.913754	-0.036564	3.550200
182.931987	4254.368458	6.918758	-0.036620	3.553447
183.374478	4262.355544	6.923763	-0.036708	3.556632
183.892481	4270.279905	6.928768	-0.036809	3.559791
184.118668	4278.299877	6.933773	-0.036857	3.562977
184.156512	4286.339305	6.938778	-0.036869	3.566162
184.470614	4294.372152	6.943782	-0.036932	3.569349
184.557706	4302.401947	6.948787	-0.036954	3.572526
184.781567	4310.431408	6.953792	-0.037001	3.575704
185.052613	4318.407729	6.958797	-0.037056	3.578860
185.108582	4326.433638	6.963802	-0.037072	3.582026
185.354909	4334.451427	6.968806	-0.037123	3.585191
185.349055	4342.494478	6.973811	-0.037127	3.588357
185.801854	4350.545244	6.978816	-0.037216	3.591535
186.104471	4358.551246	6.983821	-0.037278	3.594689
186.019217	4366.569689	6.988826	-0.037267	3.597834
186.210914	4374.608155	6.993830	-0.037308	3.600992
186.472002	4382.566770	6.998835	-0.037362	3.604118
186.707367	4390.625179	7.003840	-0.037411	3.607279
187.018784	4398.643109	7.008845	-0.037474	3.610424
187.090667	4406.699340	7.013850	-0.037493	3.613574
187.511922	4414.743042	7.018854	-0.037576	3.616726
187.554403	4422.707452	7.023859	-0.037589	3.619835
187.726015	4430.754704	7.028864	-0.037626	3.622976
188.139410	4438.772231	7.033869	-0.037708	3.626110
188.154077	4446.801946	7.038874	-0.037716	3.629234
188.475133	4454.880163	7.043878	-0.037781	3.632384
188.599632	4462.903453	7.048883	-0.037810	3.635503
188.816348	4470.912095	7.053888	-0.037855	3.638617
189.084245	4478.920180	7.058893	-0.037910	3.641730
189.153995	4486.904392	7.063898	-0.037928	3.644825
189.344528	4494.957427	7.068902	-0.037969	3.647947
189.540999	4502.971830	7.073907	-0.038011	3.651052
189.855696	4511.025585	7.078912	-0.038075	3.654172
189.975272	4519.074425	7.083917	-0.038102	3.657283
190.081914	4527.050082	7.088922	-0.038127	3.660363
190.462235	4535.082271	7.093926	-0.038203	3.663468
190.694381	4543.076188	7.098931	-0.038251	3.666553
190.997940	4551.108725	7.103936	-0.038313	3.669652
191.187845	4559.180102	7.108941	-0.038354	3.672760
191.389910	4567.186866	7.113946	-0.038396	3.675840
191.684912	4575.216292	7.118950	-0.038456	3.678930
191.851727	4583.219491	7.123955	-0.038493	3.682003
192.471643	4591.181027	7.128960	-0.038613	3.685069
192.654395	4599.249008	7.133965	-0.038652	3.688162
192.739990	4607.279554	7.138970	-0.038673	3.691236
193.070626	4615.330351	7.143974	-0.038740	3.694321
193.505941	4623.316644	7.148979	-0.038826	3.697382
193.651689	4631.335807	7.153984	-0.038859	3.700445
193.708067	4639.364160	7.158989	-0.038874	3.703507
194.106821	4647.384610	7.163994	-0.038954	3.706572
194.129778	4655.421961	7.168998	-0.038963	3.709632
194.398631	4663.501211	7.174003	-0.039018	3.712711
194.433991	4671.569253	7.179008	-0.039030	3.715777
194.684324	4679.539049	7.184013	-0.039082	3.718809
194.736509	4687.534566	7.189018	-0.039097	3.721843
194.998247	4695.524268	7.194022	-0.039151	3.724878
195.104919	4703.536115	7.199027	-0.039176	3.727914
195.392945	4711.567963	7.204032	-0.039235	3.730961
195.613417	4719.633853	7.209037	-0.039281	3.734015
195.874762	4727.631160	7.214042	-0.039335	3.737043
196.076694	4735.634619	7.219046	-0.039377	3.740069
196.161338	4743.637825	7.224051	-0.039398	3.743089
196.456470	4751.690104	7.229056	-0.039458	3.746131
196.550009	4759.719139	7.234061	-0.039481	3.749156
196.811167	4767.736150	7.239066	-0.039535	3.752179
197.070361	4775.805561	7.244070	-0.039588	3.755218
197.173145	4783.768086	7.249075	-0.039612	3.758212
197.449181	4791.782263	7.254080	-0.039669	3.761226
197.651005	4799.824137	7.259085	-0.039712	3.764246
197.688176	4807.864977	7.264090	-0.039724	3.767260
197.901982	4815.881661	7.269094	-0.039769	3.770267
197.980675	4823.919605	7.274099	-0.039789	3.773276
198.174074	4831.939623	7.279104	-0.039830	3.776278
198.632759	4839.932793	7.284109	-0.039920	3.779274
198.879981	4847.976001	7.289114	-0.039972	3.782282
198.906293	4855.986842	7.294118	-0.039982	3.785270
199.053800	4864.042162	7.299123	-0.040014	3.788275
199.299988	4872.051190	7.304128	-0.040065	3.791262
199.527414	4880.124831	7.309133	-0.040113	3.794271
199.727265	4888.109136	7.314138	-0.040155	3.797243
200.063764	4896.112880	7.319142	-0.040223	3.800223
200.376112	4904.078177	7.324147	-0.040286	3.803187
200.512518	4912.123975	7.329152	-0.040317	3.806173
200.783774	4920.130486	7.334157	-0.040372	3.809146
200.847214	4928.169616	7.339162	-0.040389	3.812124
201.158206	4936.204318	7.344166	-0.040452	3.815104
201.219753	4944.234285	7.349171	-0.040469	3.818073
201.700652	4952.217182	7.354176	-0.040564	3.821033
201.760974	4960.245466	7.359181	-0.040580	3.823997
201.912813	4968.257080	7.364186	-0.040614	3.826955
202.290137	4976.291982	7.369190	-0.040689	3.829924
202.216385	4984.355106	7.374195	-0.040680	3.832892
202.482834	4992.387686	7.379200	-0.040735	3.835853
202.706631	5000.356761	7.384205	-0.040782	3.838788
203.172606	5008.378154	7.389210	-0.040874	3.841745
203.080769	5016.376267	7.394214	-0.040862	3.844679
203.292428	5024.403810	7.399219	-0.040907	3.847628
203.340046	5032.427841	7.404224	-0.040921	3.850570
203.672708	5040.472343	7.409229	-0.040988	3.853523
203.649162	5048.528861	7.414234	-0.040989	3.856471
203.893388	5056.525808	7.419238	-0.041039	3.859401
204.070908	5064.539379	7.424243	-0.041077	3.862333
204.038148	5072.563577	7.429248	-0.041076	3.865262
204.182847	5080.609180	7.434253	-0.041109	3.868200
204.499920	5088.616655	7.439258	-0.041173	3.871126
204.626937	5096.882187	7.444262	-0.041202	3.874140
204.670794	5104.842893	7.449267	-0.041215	3.877038
205.103603	5112.725533	7.454272	-0.041301	3.879914
205.175795	5120.775796	7.459277	-0.041319	3.882842
205.332443	5128.730583	7.464282	-0.041354	3.885734
205.730201	5136.762269	7.469286	-0.041433	3.888656
205.927546	5144.781308	7.474291	-0.041475	3.891568
206.088484	5152.797988	7.479296	-0.041510	3.894476
206.569052	5160.826680	7.484301	-0.041604	3.897393
206.711596	5168.803008	7.489306	-0.041636	3.900281
206.765677	5176.844261	7.494310	-0.041651	3.903190
206.793224	5184.865235	7.499315	-0.041662	3.906088
207.083674	5192.852017	7.504320	-0.041721	3.908977
207.559951	5200.931536	7.509325	-0.041815	3.911901
207.547100	5208.944921	7.514330	-0.041818	3.914789
207.734990	5216.967158	7.519334	-0.041858	3.917682
207.986916	5224.923665	7.524339	-0.041910	3.920551
208.108651	5232.950774	7.529344	-0.041938	3.923440
208.210428	5240.998752	7.534349	-0.041962	3.926335
208.531088	5248.984513	7.539354	-0.042026	3.929208
208.973945	5257.027688	7.544358	-0.042114	3.932103
208.815175	5265.084701	7.549363	-0.042090	3.934989
209.121328	5273.094371	7.554368	-0.042152	3.937865
209.329773	5281.100830	7.559373	-0.042196	3.940736
209.521631	5289.086096	7.564378	-0.042237	3.943596
209.833037	5297.125638	7.569382	-0.042300	3.946476
210.004364	5305.130721	7.574387	-0.042337	3.949340
209.984009	5313.211217	7.579392	-0.042338	3.952224
210.092289	5321.253848	7.584397	-0.042364	3.955096
210.590527	5329.200658	7.589402	-0.042462	3.957937
210.829349	5337.218251	7.594406	-0.042511	3.960798
210.986316	5345.201736	7.599411	-0.042546	3.963642
211.221886	5353.239145	7.604416	-0.042595	3.966506
211.501769	5361.273374	7.609421	-0.042652	3.969366
211.732151	5369.277140	7.614426	-0.042700	3.972213
212.171908	5377.334257	7.619430	-0.042787	3.975081
212.420548	5385.316382	7.624435	-0.042838	3.977916
212.618193	5393.335730	7.629440	-0.042880	3.980762
212.855783	5401.368782	7.634445	-0.042930	3.983611
212.980740	5409.399580	7.639450	-0.042958	3.986455
213.269181	5417.428772	7.644454	-0.043017	3.989300
213.476355	5425.472790	7.649459	-0.043061	3.992146
213.665637	5433.482770	7.654464	-0.043101	3.994978
214.038096	5441.508035	7.659469	-0.043176	3.997816
214.039439	5449.500774	7.664474	-0.043181	4.000635
214.428540	5457.524520	7.669478	-0.043259	4.003469
214.292059	5465.590601	7.674483	-0.043238	4.006307
214.606258	5473.573348	7.679488	-0.043302	4.009122
214.754952	5481.633905	7.684493	-0.043335	4.011959
214.944406	5489.628258	7.689498	-0.043375	4.014771
215.371835	5497.648234	7.694502	-0.043460	4.017594
215.366250	5505.648209	7.699507	-0.043464	4.020401
215.761201	5513.703385	7.704512	-0.043543	4.023232
215.941349	5521.740610	7.709517	-0.043582	4.026051
216.060228	5529.722836	7.714522	-0.043609	4.028848
216.480308	5537.810370	7.719526	-0.043692	4.031684
216.571116	5545.893542	7.724531	-0.043714	4.034512
216.637341	5553.874426	7.729536	-0.043732	4.037302
216.824083	5561.854046	7.734541	-0.043772	4.040091
216.942639	5569.831359	7.739546	-0.043799	4.042877
217.164505	5577.858322	7.744550	-0.043846	4.045679
217.416855	5585.843092	7.749555	-0.043898	4.048465
217.650236	5593.858468	7.754560	-0.043946	4.051260
217.980848	5601.886291	7.759565	-0.044013	4.054058
217.891185	5609.936852	7.764570	-0.044001	4.056856
218.304021	5617.916040	7.769574	-0.044083	4.059635
218.606521	5625.943979	7.774579	-0.044145	4.062427
218.692760	5633.940320	7.779584	-0.044166	4.065203
218.793546	5642.017242	7.784589	-0.044190	4.068005
218.887250	5649.999127	7.789594	-0.044213	4.070772
219.403554	5658.057326	7.794598	-0.044314	4.073570
219.571287	5666.086214	7.799603	-0.044350	4.076351
219.894892	5674.042340	7.804608	-0.044416	4.079107
220.283768	5682.085500	7.809613	-0.044493	4.081891
220.296697	5690.053878	7.814618	-0.044501	4.084644
220.486348	5698.123115	7.819622	-0.044541	4.087431
220.501328	5706.096857	7.824627	-0.044549	4.090181
220.607577	5714.162222	7.829632	-0.044574	4.092962
220.725407	5722.167397	7.834637	-0.044601	4.095721
220.976634	5730.143973	7.839642	-0.044653	4.098469
221.416469	5738.223381	7.844646	-0.044740	4.101254
221.587140	5746.191278	7.849651	-0.044777	4.103995
221.675703	5754.242179	7.854656	-0.044799	4.106761
221.827126	5762.268032	7.859661	-0.044832	4.109518
221.988413	5770.297163	7.864666	-0.044868	4.112274
222.209279	5778.347806	7.869670	-0.044914	4.115036
222.363479	5786.380846	7.874675	-0.044948	4.117790
222.767991	5794.305397	7.879680	-0.045028	4.120508
222.888272	5802.366049	7.884685	-0.045056	4.123266
223.033903	5810.339898	7.889690	-0.045088	4.125994
223.270296	5818.422831	7.894694	-0.045137	4.128758
223.408819	5826.414112	7.899699	-0.045168	4.131488
223.426834	5834.493691	7.904704	-0.045177	4.134245
223.714121	5842.527155	7.909709	-0.045235	4.136987
223.770014	5850.473269	7.914714	-0.045251	4.139695
224.033342	5858.533037	7.919718	-0.045305	4.142443
224.143830	5866.502548	7.924723	-0.045331	4.145156
224.286188	5874.557989	7.929728	-0.045362	4.147897
224.283907	5882.583286	7.934733	-0.045367	4.150624
224.308129	5890.611135	7.939738	-0.045377	4.153350
224.665966	5898.645069	7.944742	-0.045449	4.156081
224.734435	5906.628694	7.949747	-0.045467	4.158789
224.798631	5914.695103	7.954752	-0.045484	4.161523
225.171961	5922.658942	7.959757	-0.045558	4.164225
225.458903	5930.655851	7.964762	-0.045617	4.166935
225.519237	5938.703313	7.969766	-0.045633	4.169658
225.564885	5946.739911	7.974771	-0.045647	4.172375
226.104785	5954.748338	7.979776	-0.045753	4.175086
226.307050	5962.806281	7.984781	-0.045795	4.177808
226.156725	5970.763187	7.989786	-0.045773	4.180491
226.566413	5978.765855	7.994790	-0.045854	4.183193
226.548897	5986.779841	7.999795	-0.045856	4.185893
226.626635	5994.809948	8.004800	-0.045876	4.188598
227.078537	6002.847634	8.009805	-0.045965	4.191307
227.282535	6010.949415	8.014810	-0.046008	4.194034
227.605489	6018.972075	8.019814	-0.046073	4.196733
227.697718	6026.896377	8.024819	-0.046096	4.199395
227.850792	6034.914180	8.029824	-0.046129	4.202087
227.898480	6042.891932	8.034829	-0.046143	4.204764
227.962788	6050.919023	8.039834	-0.046160	4.207455
228.436325	6058.905627	8.044838	-0.046254	4.210135
228.712593	6066.988212	8.049843	-0.046310	4.212843
228.756027	6074.998890	8.054848	-0.046324	4.215523
228.901747	6083.014531	8.059853	-0.046356	4.218204
229.019133	6090.996895	8.064858	-0.046383	4.220872
229.426676	6098.998523	8.069862	-0.046464	4.223548
229.624610	6107.051592	8.074867	-0.046506	4.226237
229.760521	6115.077912	8.079872	-0.046536	4.228915
230.020380	6123.133091	8.084877	-0.046590	4.231602
229.910451	6131.150328	8.089882	-0.046575	4.234271
230.276431	6139.155702	8.094886	-0.046648	4.236938
230.310759	6147.103066	8.099891	-0.046659	4.239582
230.521371	6155.149267	8.104896	-0.046704	4.242258
230.820435	6163.163470	8.109901	-0.046765	4.244923
230.888318	6171.194681	8.114906	-0.046783	4.247590
231.080945	6179.229537	8.119910	-0.046824	4.250258
231.300466	6187.237734	8.124915	-0.046870	4.252915
231.710585	6195.251696	8.129920	-0.046951	4.255574
231.728007	6203.298981	8.134925	-0.046960	4.258239
231.741920	6211.300453	8.139930	-0.046967	4.260887
232.142712	6219.299834	8.144934	-0.047047	4.263536
232.266947	6227.331237	8.149939	-0.047075	4.266191
232.549092	6235.358990	8.154944	-0.047133	4.268845
232.538384	6243.426630	8.159949	-0.047136	4.271509
232.781006	6251.451362	8.164954	-0.047187	4.274158
233.003967	6259.487348	8.169958	-0.047233	4.276809
233.134961	6267.414084	8.174963	-0.047263	4.279422
233.351014	6275.469800	8.179968	-0.047308	4.282076
233.699698	6283.446755	8.184973	-0.047378	4.284704
233.757197	6291.487931	8.189978	-0.047394	4.287349
233.980298	6299.498828	8.194982	-0.047441	4.289984
234.019408	6307.524771	8.199987	-0.047453	4.292620
234.239306	6315.552416	8.204992	-0.047499	4.295257
234.474084	6323.595219	8.209997	-0.047548	4.297897
234.635087	6331.548552	8.215002	-0.047583	4.300506
234.771684	6339.588355	8.220006	-0.047614	4.303141
234.872801	6347.600568	8.225011	-0.047638	4.305766
235.053094	6355.663668	8.230016	-0.047677	4.308406
235.415171	6363.676215	8.235021	-0.047749	4.311029
235.473764	6371.711907	8.240026	-0.047765	4.313656
235.516990	6379.714618	8.245030	-0.047778	4.316270
235.836981	6387.677991	8.250035	-0.047843	4.318872
236.030154	6395.706437	8.255040	-0.047884	4.321492
236.290126	6403.714488	8.260045	-0.047938	4.324105
236.240681	6411.741632	8.265050	-0.047934	4.326721
236.647933	6419.744021	8.270054	-0.048015	4.329329
236.674189	6427.812004	8.275059	-0.048025	4.331955
236.960080	6435.787449	8.280064	-0.048083	4.334551
237.312206	6443.858696	8.285069	-0.048154	4.337177
237.457305	6451.790105	8.290074	-0.048186	4.339755
237.692206	6459.835142	8.295078	-0.048235	4.342368
237.889532	6467.852174	8.300083	-0.048277	4.344970
238.035828	6475.860642	8.305088	-0.048309	4.347568
238.261784	6483.909060	8.310093	-0.048357	4.350178
238.298668	6491.979491	8.315098	-0.048369	4.352792
238.573147	6500.011750	8.320102	-0.048425	4.355394
238.508361	6507.998265	8.325107	-0.048418	4.357977
238.715736	6515.966150	8.330112	-0.048462	4.360554
238.917004	6523.965047	8.335117	-0.048504	4.363140
239.027256	6531.956874	8.340122	-0.048530	4.365721
239.189899	6540.002871	8.345126	-0.048565	4.368318
239.455731	6548.043203	8.350131	-0.048620	4.370913
239.565429	6556.051417	8.355136	-0.048646	4.373495
239.736268	6564.075967	8.360141	-0.048683	4.376081
239.887817	6572.035827	8.365146	-0.048716	4.378644
240.211415	6580.106238	8.370150	-0.048781	4.381243
240.336771	6588.086777	8.375155	-0.048810	4.383810
240.450153	6596.105288	8.380160	-0.048836	4.386387
240.762592	6604.137985	8.385165	-0.048900	4.388969
240.825162	6612.115331	8.390170	-0.048916	4.391530
240.925280	6620.188279	8.395174	-0.048940	4.394120
241.166245	6628.237541	8.400179	-0.048990	4.396702
241.370223	6636.210340	8.405184	-0.049033	4.399258
241.419421	6644.273112	8.410189	-0.049048	4.401840
241.471201	6652.197168	8.415194	-0.049062	4.404376
241.749096	6660.264037	8.420198	-0.049119	4.406958
241.987915	6668.260127	8.425203	-0.049169	4.409515
242.166349	6676.315596	8.430208	-0.049207	4.412089
242.520595	6684.394865	8.435213	-0.049279	4.414671
242.734474	6692.383118	8.440218	-0.049323	4.417221
242.889959	6700.371013	8.445222	-0.049358	4.419769
242.951276	6708.384467	8.450227	-0.049374	4.422323
243.237265	6716.354470	8.455232	-0.049433	4.424863
243.317516	6724.467267	8.460237	-0.049453	4.427447
243.489665	6732.424640	8.465242	-0.049490	4.429979
243.726802	6740.504637	8.470246	-0.049539	4.432550
243.900482	6748.518498	8.475251	-0.049577	4.435097
244.037589	6756.509969	8.480256	-0.049607	4.437636
244.269723	6764.499994	8.485261	-0.049656	4.440173
244.339707	6772.522239	8.490266	-0.049674	4.442719
244.417626	6780.515539	8.495270	-0.049694	4.445253
244.479253	6788.559948	8.500275	-0.049710	4.447803
244.700902	6796.544061	8.505280	-0.049757	4.450332
244.949621	6804.608476	8.510285	-0.049808	4.452886
245.003040	6812.587983	8.515290	-0.049823	4.455410
245.324695	6820.659998	8.520294	-0.049888	4.457963
245.513164	6828.602800	8.525299	-0.049928	4.460474
245.750646	6836.613921	8.530304	-0.049978	4.463004
246.074624	6844.658485	8.535309	-0.050043	4.465544
246.147876	6852.682578	8.540314	-0.050062	4.468076
246.449930	6860.725833	8.545318	-0.050124	4.470612
246.653289	6868.770777	8.550323	-0.050167	4.473148
246.804928	6876.772272	8.555328	-0.050200	4.475668
246.991779	6884.787939	8.560333	-0.050240	4.478191
246.969200	6892.706862	8.565338	-0.050241	4.480682
247.315323	6900.763990	8.570343	-0.050310	4.483216
247.517219	6908.785333	8.575347	-0.050353	4.485736
247.516096	6916.809029	8.580352	-0.050358	4.488256
247.890740	6924.816198	8.585357	-0.050433	4.490770
247.957479	6932.837485	8.590362	-0.050451	4.493286
247.973790	6940.887612	8.595367	-0.050459	4.495809
247.925272	6948.881974	8.600371	-0.050455	4.498314
248.279063	6956.866772	8.605376	-0.050526	4.500815
248.466221	6964.937216	8.610381	-0.050566	4.503341
248.447311	6972.922888	8.615386	-0.050568	4.505838
248.909456	6980.945608	8.620391	-0.050659	4.508347
249.210865	6989.001064	8.625395	-0.050720	4.510864
249.050879	6997.001167	8.630400	-0.050695	4.513362
249.361343	7005.036672	8.635405	-0.050758	4.515870
249.564175	7012.985323	8.640410	-0.050801	4.518350
249.610387	7020.995467	8.645415	-0.050815	4.520847
249.793146	7029.005265	8.650419	-0.050854	4.523342
249.902570	7037.001924	8.655424	-0.050880	4.525832
250.267141	7045.057859	8.660429	-0.050953	4.528340
250.251166	7053.020985	8.665434	-0.050955	4.530817
250.471176	7061.113872	8.670439	-0.051001	4.533333
250.682471	7069.121931	8.675443	-0.051046	4.535821
250.711587	7077.099111	8.680448	-0.051056	4.538298
250.967781	7085.130987	8.685453	-0.051109	4.540791
251.193223	7093.109119	8.690458	-0.051156	4.543266
251.369395	7101.174502	8.695463	-0.051194	4.545766
251.488518	7109.214382	8.700467	-0.051222	4.548257
251.636553	7117.190040	8.705472	-0.051254	4.550727
251.761608	7125.279156	8.710477	-0.051283	4.553231
251.960027	7133.253408	8.715482	-0.051325	4.555697
252.377222	7141.281914	8.720487	-0.051408	4.558180
252.545941	7149.261092	8.725491	-0.051444	4.560645
252.468686	7157.269582	8.730496	-0.051435	4.563118
252.790235	7165.274337	8.735501	-0.051500	4.565589
252.857952	7173.293244	8.740506	-0.051518	4.568062
253.084861	7181.331399	8.745511	-0.051565	4.570541
253.238837	7189.398474	8.750515	-0.051599	4.573026
253.529715	7197.356205	8.755520	-0.051658	4.575477
253.652834	7205.399738	8.760525	-0.051686	4.577953
253.667496	7213.359499	8.765530	-0.051694	4.580401
253.710974	7221.447419	8.770535	-0.051708	4.582888
254.125386	7229.395123	8.775539	-0.051790	4.585330
254.342221	7237.429731	8.780544	-0.051835	4.587798
254.451782	7245.499329	8.785549	-0.051861	4.590275
254.510506	7253.505151	8.790554	-0.051877	4.592731
254.725476	7261.593698	8.795559	-0.051922	4.595211
254.907337	7269.598049	8.800563	-0.051961	4.597664
254.899767	7277.532266	8.805568	-0.051965	4.600094
255.383155	7285.563762	8.810573	-0.052060	4.602553
255.442776	7293.477991	8.815578	-0.052076	4.604974
255.565891	7301.559868	8.820583	-0.052104	4.607446
255.739716	7309.584891	8.825587	-0.052142	4.609898
256.026920	7317.626677	8.830592	-0.052201	4.612355
255.884447	7325.690642	8.835597	-0.052179	4.614817
255.981487	7333.677397	8.840602	-0.052203	4.617254
256.242713	7341.626744	8.845607	-0.052256	4.619678
256.378446	7349.688712	8.850611	-0.052287	4.622135
256.648147	7357.611829	8.855616	-0.052342	4.624549
257.096726	7365.730400	8.860621	-0.052431	4.627021
257.059452	7373.708539	8.865626	-0.052429	4.629449
257.215250	7381.771495	8.870631	-0.052463	4.631901
257.551491	7389.800310	8.875635	-0.052531	4.634341
257.761831	7397.804308	8.880640	-0.052575	4.636773
257.981244	7405.791034	8.885645	-0.052621	4.639198
258.032185	7413.812284	8.890650	-0.052636	4.641633
258.113126	7421.773034	8.895655	-0.052656	4.644048
258.094498	7429.805542	8.900659	-0.052658	4.646483
258.199905	7437.811876	8.905664	-0.052683	4.648909
258.638196	7445.920836	8.910669	-0.052769	4.651365
258.824547	7453.870101	8.915674	-0.052809	4.653771
258.894587	7461.943758	8.920679	-0.052827	4.656214
259.244926	7469.911569	8.925683	-0.052898	4.658623
259.320328	7477.920442	8.930688	-0.052917	4.661043
259.666184	7485.986669	8.935693	-0.052987	4.663479
259.698536	7493.952065	8.940698	-0.052998	4.665884
260.198744	7501.983296	8.945703	-0.053096	4.668307
260.341543	7509.980516	8.950707	-0.053128	4.670718
260.417908	7518.050927	8.955712	-0.053147	4.673151
260.606933	7526.149106	8.960717	-0.053188	4.675591
260.792523	7534.083576	8.965722	-0.053227	4.677980
260.895195	7542.025766	8.970727	-0.053251	4.680370
261.087503	7550.031863	8.975731	-0.053292	4.682778
261.127111	7557.982901	8.980736	-0.053305	4.685168
261.344591	7566.095212	8.985741	-0.053351	4.687606
261.512436	7574.054465	8.990746	-0.053387	4.689996
261.817576	7582.129186	8.995751	-0.053449	4.692419
261.951885	7590.164172	9.000755	-0.053479	4.694830
261.986144	7598.183786	9.005760	-0.053491	4.697234
262.074426	7606.120467	9.010765	-0.053512	4.699613
262.323144	7614.169951	9.015770	-0.053564	4.702024
262.426678	7622.157736	9.020775	-0.053588	4.704415
262.838514	7630.212918	9.025779	-0.053670	4.706825
263.145688	7638.193135	9.030784	-0.053732	4.709211
263.152867	7646.269776	9.035789	-0.053739	4.711626
263.217407	7654.283187	9.040794	-0.053756	4.714020
263.469829	7662.322403	9.045799	-0.053808	4.716420
263.588740	7670.288122	9.050803	-0.053835	4.718798
263.672794	7678.250232	9.055808	-0.053856	4.721173
264.130997	7686.351163	9.060813	-0.053947	4.723587
264.186326	7694.346355	9.065818	-0.053962	4.725970
264.273781	7702.392082	9.070823	-0.053984	4.728366
264.260370	7710.393632	9.075827	-0.053986	4.730749
264.346981	7718.403479	9.080832	-0.054008	4.733132
264.716608	7726.452105	9.085837	-0.054082	4.735525
264.713473	7734.429230	9.090842	-0.054086	4.737896
265.115150	7742.460291	9.095847	-0.054166	4.740281
265.398450	7750.517284	9.100851	-0.054224	4.742673
265.298485	7758.442316	9.105856	-0.054211	4.745025
265.522994	7766.522602	9.110861	-0.054258	4.747422
265.748952	7774.488081	9.115866	-0.054305	4.749783
266.018581	7782.528768	9.120871	-0.054360	4.752165
266.105866	7790.615527	9.125875	-0.054382	4.754560
266.307514	7798.558132	9.130880	-0.054424	4.756911
266.391072	7806.571774	9.135885	-0.054445	4.759282
266.355324	7814.540335	9.140890	-0.054443	4.761640
266.846603	7822.517932	9.145895	-0.054540	4.763996
267.045231	7830.589674	9.150899	-0.054582	4.766380
266.989970	7838.579497	9.155904	-0.054577	4.768740
267.163862	7846.660106	9.160909	-0.054615	4.771125
267.295833	7854.674371	9.165914	-0.054644	4.773489
267.362619	7862.689593	9.170919	-0.054662	4.775852
267.603121	7870.683854	9.175923	-0.054712	4.778207
267.983290	7878.639741	9.180928	-0.054788	4.780550
267.975950	7886.695587	9.185933	-0.054792	4.782922
268.185818	7894.632524	9.190938	-0.054836	4.785257
268.595004	7902.748522	9.195943	-0.054917	4.787642
268.589933	7910.740028	9.200947	-0.054921	4.789992
268.825882	7918.792461	9.205952	-0.054970	4.792357
268.997238	7926.811774	9.210957	-0.055008	4.794712
269.163048	7934.836076	9.215962	-0.055044	4.797066
269.481724	7942.771152	9.220967	-0.055108	4.799393
269.411586	7950.856995	9.225971	-0.055100	4.801765
269.572945	7958.776048	9.230976	-0.055135	4.804086
269.870211	7966.869737	9.235981	-0.055196	4.806456
269.966290	7974.839278	9.240986	-0.055219	4.808789
270.174190	7982.904321	9.245991	-0.055263	4.811149
270.344030	7990.413425	9.250995	-0.055299	4.813345
270.268265	7995.114473	9.256000	-0.055288	4.814720

270.469471	7997.749026	9.261005	-0.055327	4.815489
270.782552	7999.153592	9.266010	-0.055386	4.815898
270.782518	7999.575428	9.271015	-0.055387	4.816021
270.874810	8000.378084	9.276019	-0.055404	4.816256
270.895010	8000.483108	9.281024	-0.055408	4.816286
271.311752	8000.511982	9.286029	-0.055485	4.816292
271.305362	8000.579147	9.291034	-0.055484	4.816312
271.287684	8000.488037	9.296039	-0.055481	4.816286
271.337003	8000.507077	9.301043	-0.055490	4.816291
271.157587	8000.495289	9.306048	-0.055456	4.816288
271.447283	8000.497306	9.311053	-0.055510	4.816287
271.673205	8000.501376	9.316058	-0.055552	4.816287
271.590758	8000.464636	9.321063	-0.055537	4.816277
271.516601	8000.589321	9.326067	-0.055523	4.816314
271.571121	8000.477085	9.331072	-0.055533	4.816281
271.893596	8000.507464	9.336077	-0.055593	4.816288
271.882580	8000.526483	9.341082	-0.055591	4.816294
271.823130	8000.483749	9.346087	-0.055580	4.816281
271.884096	8000.498728	9.351091	-0.055591	4.816286
271.804392	8000.568842	9.356096	-0.055576	4.816306
271.850691	8000.507724	9.361101	-0.055585	4.816288
271.893064	8000.580042	9.366106	-0.055593	4.816309
272.281716	8000.603073	9.371111	-0.055665	4.816314
272.087603	8000.411583	9.376115	-0.055629	4.816259
272.121859	8000.520069	9.381120	-0.055635	4.816291
272.148469	8000.522678	9.386125	-0.055640	4.816291
272.176172	8000.587256	9.391130	-0.055645	4.816310
272.378610	8000.504390	9.396135	-0.055683	4.816285
272.256134	8000.422068	9.401139	-0.055660	4.816261
272.080719	8000.487251	9.406144	-0.055627	4.816281
272.324309	8000.518343	9.411149	-0.055672	4.816289
272.378714	8000.484072	9.416154	-0.055682	4.816279
272.459049	8000.518626	9.421159	-0.055697	4.816288
272.354280	8000.572268	9.426163	-0.055678	4.816305
272.293811	8000.491064	9.431168	-0.055666	4.816281
272.428288	8000.521255	9.436173	-0.055691	4.816289
272.388269	8000.503437	9.441178	-0.055684	4.816284
272.324931	8000.501219	9.446183	-0.055672	4.816284
272.445164	8000.581352	9.451187	-0.055694	4.816307
272.607533	8000.569324	9.456192	-0.055724	4.816302
272.542824	8000.501928	9.461197	-0.055712	4.816283
272.600912	8000.590553	9.466202	-0.055723	4.816309
272.583369	8000.505851	9.471207	-0.055720	4.816284
272.562997	8000.510817	9.476211	-0.055716	4.816286
272.539710	8000.592632	9.481216	-0.055711	4.816310
272.699092	8000.490831	9.486221	-0.055741	4.816279
272.670842	8000.493519	9.491226	-0.055736	4.816280
272.591378	8000.525188	9.496231	-0.055721	4.816290
272.753631	8000.553745	9.501235	-0.055751	4.816297
272.441181	8000.474400	9.506240	-0.055693	4.816276
272.574606	8000.498163	9.511245	-0.055718	4.816282
272.853367	8000.585432	9.516250	-0.055769	4.816306
272.980044	8000.516151	9.521255	-0.055793	4.816285
272.934961	8000.515330	9.526259	-0.055784	4.816285
272.750295	8000.596368	9.531264	-0.055750	4.816310
273.007757	8000.421572	9.536269	-0.055798	4.816257
272.969026	8000.597100	9.541274	-0.055791	4.816309
272.774158	8000.501719	9.546279	-0.055754	4.816282
272.845904	8000.490191	9.551283	-0.055767	4.816278
273.020627	8000.518973	9.556288	-0.055800	4.816286
273.074669	8000.595777	9.561293	-0.055810	4.816308
272.934417	8000.509927	9.566298	-0.055784	4.816283
273.008315	8000.519799	9.571303	-0.055797	4.816286
272.953232	8000.404513	9.576307	-0.055787	4.816252
272.930534	8000.587807	9.581312	-0.055783	4.816306
272.944498	8000.528240	9.586317	-0.055785	4.816289
272.957384	8000.514581	9.591322	-0.055788	4.816285
273.049003	8000.506616	9.596327	-0.055805	4.816282
273.119587	8000.595467	9.601331	-0.055818	4.816307
272.977842	8000.599309	9.606336	-0.055791	4.816309
273.098003	8000.520297	9.611341	-0.055814	4.816286
272.945593	8000.502585	9.616346	-0.055785	4.816281
273.157002	8000.581163	9.621351	-0.055825	4.816303
273.207556	8000.576729	9.626355	-0.055834	4.816301
273.205529	8000.579890	9.631360	-0.055833	4.816302
273.268204	8000.517997	9.636365	-0.055845	4.816284
273.171884	8000.515183	9.641370	-0.055827	4.816284
273.263989	8000.502955	9.646375	-0.055844	4.816280
273.174260	8000.458604	9.651379	-0.055827	4.816267
273.214391	8000.393101	9.656384	-0.055835	4.816248
273.308375	8000.397995	9.661389	-0.055852	4.816249
273.244847	8000.599779	9.666394	-0.055840	4.816308
273.211986	8000.512663	9.671399	-0.055834	4.816283
273.392932	8000.514856	9.676403	-0.055868	4.816282
273.356139	8000.600701	9.681408	-0.055861	4.816308
273.465302	8000.520422	9.686413	-0.055881	4.816284
273.255778	8000.487793	9.691418	-0.055842	4.816275
273.333820	8000.496672	9.696423	-0.055856	4.816277
273.326052	8000.515751	9.701427	-0.055855	4.816283
273.376288	8000.512379	9.706432	-0.055864	4.816282
273.562686	8000.393976	9.711437	-0.055899	4.816246
273.438486	8000.527375	9.716442	-0.055876	4.816286
273.493983	8000.495259	9.721447	-0.055886	4.816276
273.535705	8000.514164	9.726451	-0.055894	4.816281
273.422451	8000.596492	9.731456	-0.055872	4.816306
273.450053	8000.525421	9.736461	-0.055877	4.816285
273.550874	8000.493056	9.741466	-0.055896	4.816275
273.386413	8000.519986	9.746471	-0.055865	4.816284
273.361782	8000.521670	9.751475	-0.055861	4.816285
273.574044	8000.491318	9.756480	-0.055900	4.816275
273.491238	8000.504769	9.761485	-0.055885	4.816279
273.344471	8000.521338	9.766490	-0.055857	4.816285
273.646464	8000.520377	9.771495	-0.055914	4.816283
273.694096	8000.609883	9.776499	-0.055922	4.816309
273.456310	8000.523338	9.781504	-0.055878	4.816285
273.633970	8000.513723	9.786509	-0.055911	4.816281
273.626790	8000.529608	9.791514	-0.055910	4.816286
273.515657	8000.507300	9.796519	-0.055889	4.816280
273.562061	8000.535902	9.801523	-0.055897	4.816288
273.606904	8000.508935	9.806528	-0.055906	4.816280
273.766319	8000.449857	9.811533	-0.055935	4.816261
273.525963	8000.394242	9.816538	-0.055890	4.816246
273.449347	8000.465482	9.821543	-0.055876	4.816268
273.681103	8000.389553	9.826547	-0.055919	4.816244
273.750406	8000.604419	9.831552	-0.055932	4.816307
273.832571	8000.213904	9.836557	-0.055947	4.816192
273.746083	8000.500721	9.841562	-0.055931	4.816276
273.774242	8000.517244	9.846567	-0.055936	4.816281
273.587447	8000.525613	9.851571	-0.055901	4.816285
273.536380	8000.602656	9.856576	-0.055892	4.816307
273.835255	8000.452104	9.861581	-0.055947	4.816262
273.580716	8000.563923	9.866586	-0.055900	4.816296
273.587487	8000.388871	9.871591	-0.055901	4.816245
273.829898	8000.494711	9.876595	-0.055946	4.816274
273.593287	8000.386826	9.881600	-0.055902	4.816244
273.602001	8000.375228	9.886605	-0.055904	4.816241
273.650179	8000.548055	9.891610	-0.055913	4.816291
273.761347	8000.418680	9.896615	-0.055933	4.816252
273.783635	8000.525886	9.901619	-0.055937	4.816284
273.505465	8000.510174	9.906624	-0.055885	4.816281
273.665210	8000.409447	9.911629	-0.055915	4.816250
273.719380	8000.591996	9.916634	-0.055925	4.816303
273.711552	8000.523489	9.921639	-0.055924	4.816283
273.904230	8000.489579	9.926643	-0.055959	4.816272
273.581373	8000.509375	9.931648	-0.055899	4.816280
273.593204	8000.512787	9.936653	-0.055901	4.816281
273.746322	8000.524090	9.941658	-0.055930	4.816283
273.746959	8000.484575	9.946663	-0.055930	4.816272
273.675755	8000.603979	9.951667	-0.055917	4.816307
273.832083	8000.454057	9.956672	-0.055946	4.816262
273.815262	8000.395001	9.961677	-0.055942	4.816245
273.748290	8000.435440	9.966682	-0.055930	4.816257
273.630984	8000.515559	9.971687	-0.055908	4.816281
273.715982	8000.423094	9.976691	-0.055924	4.816254
273.605767	8000.490524	9.981696	-0.055903	4.816274
273.621827	8000.401087	9.986701	-0.055906	4.816248
273.684970	8000.519711	9.991706	-0.055918	4.816282
273.715019	8000.385667	9.996711	-0.055923	4.816243
273.683416	8000.380817	10.001715	-0.055917	4.816242
273.658456	8000.409198	10.006720	-0.055912	4.816250
274.029417	8000.217225	10.011725	-0.055981	4.816192
273.846761	8000.420063	10.016730	-0.055947	4.816252
273.927269	8000.345675	10.021735	-0.055962	4.816230
274.041249	8000.416085	10.026739	-0.055983	4.816250
273.908786	8000.612354	10.031744	-0.055959	4.816308
274.038111	8000.265413	10.036749	-0.055983	4.816206
273.989834	8000.511266	10.041754	-0.055974	4.816278
273.820878	8000.407806	10.046759	-0.055942	4.816249
273.815498	8000.403430	10.051763	-0.055941	4.816248
273.806480	8000.442780	10.056768	-0.055939	4.816259
273.872385	8000.371333	10.061773	-0.055952	4.816238
273.780392	8000.502109	10.066778	-0.055934	4.816277
273.895296	8000.450773	10.071783	-0.055956	4.816261
273.974351	8000.379563	10.076787	-0.055970	4.816240
273.939104	8000.607495	10.081792	-0.055964	4.816307
273.805274	8000.438446	10.086797	-0.055939	4.816258
273.917038	8000.513089	10.091802	-0.055960	4.816279
274.036538	8000.481062	10.096807	-0.055982	4.816269
274.186346	8000.285093	10.101811	-0.056009	4.816211
274.007407	8000.511497	10.106816	-0.055976	4.816278
273.992718	8000.269834	10.111821	-0.055973	4.816208
273.960765	8000.537344	10.116826	-0.055967	4.816286
273.823298	8000.561557	10.121831	-0.055942	4.816294
274.014868	8000.499856	10.126835	-0.055977	4.816275
273.927822	8000.519639	10.131840	-0.055961	4.816281
273.904407	8000.510665	10.136845	-0.055957	4.816279
273.913757	8000.504418	10.141850	-0.055958	4.816277
273.969131	8000.380444	10.146855	-0.055968	4.816240
274.024284	8000.439111	10.151859	-0.055979	4.816257
273.975923	8000.499113	10.156864	-0.055970	4.816275
274.180157	8000.344715	10.161869	-0.056007	4.816229
274.163644	8000.407429	10.166874	-0.056004	4.816247
273.930330	8000.338054	10.171879	-0.055961	4.816228
274.185245	8000.441985	10.176883	-0.056008	4.816257
273.976552	8000.396553	10.181888	-0.055969	4.816245
273.853867	8000.314223	10.186893	-0.055946	4.816222
273.994512	8000.483380	10.191898	-0.055973	4.816270
273.906227	8000.393126	10.196903	-0.055956	4.816244
274.108369	8000.417065	10.201907	-0.055994	4.816250
274.102592	8000.361412	10.206912	-0.055992	4.816234
273.980612	8000.482034	10.211917	-0.055970	4.816270
274.238520	8000.501640	10.216922	-0.056018	4.816274
273.977153	8000.512934	10.221927	-0.055969	4.816279
274.075190	8000.415364	10.226931	-0.055987	4.816250
274.006901	8000.495300	10.231936	-0.055974	4.816274
273.962712	8000.388753	10.236941	-0.055966	4.816243
273.894644	8000.517825	10.241946	-0.055953	4.816281
273.954816	8000.490067	10.246951	-0.055964	4.816272
274.020751	8000.507273	10.251955	-0.055977	4.816277
273.961409	8000.508330	10.256960	-0.055966	4.816278
274.170880	8000.512108	10.261965	-0.056004	4.816278
274.258722	8000.527573	10.266970	-0.056021	4.816282
274.128586	8000.455789	10.271975	-0.055996	4.816261
274.356424	8000.451353	10.276979	-0.056039	4.816259
274.306001	8000.441890	10.281984	-0.056029	4.816256
274.325208	8000.284151	10.286989	-0.056033	4.816210
274.208317	8000.522357	10.291994	-0.056011	4.816281
274.107113	8000.530135	10.296999	-0.055992	4.816283
274.062906	8000.421451	10.302003	-0.055984	4.816252
274.126925	8000.596703	10.307008	-0.055996	4.816303
274.234463	8000.307045	10.312013	-0.056015	4.816217
274.250108	8000.403450	10.317018	-0.056018	4.816246
274.184173	8000.499451	10.322023	-0.056006	4.816274
274.283086	8000.525798	10.327027	-0.056024	4.816281
274.224868	8000.602712	10.332032	-0.056014	4.816304
274.143745	8000.419660	10.337037	-0.055998	4.816251
274.230204	8000.531231	10.342042	-0.056014	4.816283
274.338671	8000.529979	10.347047	-0.056035	4.816282
274.458799	8000.400765	10.352051	-0.056057	4.816244
274.360373	8000.602990	10.357056	-0.056039	4.816303
274.324103	8000.419680	10.362061	-0.056032	4.816250
274.214868	8000.513831	10.367066	-0.056011	4.816278
274.307299	8000.513358	10.372071	-0.056028	4.816277
274.274244	8000.399534	10.377075	-0.056022	4.816244
274.013503	8000.531535	10.382080	-0.055974	4.816284
274.140865	8000.408861	10.387085	-0.055997	4.816248
274.224273	8000.388998	10.392090	-0.056013	4.816242
274.327179	8000.427166	10.397095	-0.056032	4.816252
274.197833	8000.399189	10.402099	-0.056007	4.816245
274.169625	8000.509756	10.407104	-0.056002	4.816277
274.085684	8000.398218	10.412109	-0.055986	4.816245
274.327463	8000.542501	10.417114	-0.056032	4.816286
274.337831	8000.514911	10.422119	-0.056033	4.816278
274.328420	8000.397242	10.427123	-0.056031	4.816243
274.380535	8000.530623	10.432128	-0.056041	4.816282
274.428678	8000.384086	10.437133	-0.056050	4.816239
274.424664	8000.371189	10.442138	-0.056049	4.816235
274.168047	8000.380433	10.447143	-0.056001	4.816239
274.305981	8000.298537	10.452147	-0.056027	4.816215
274.043421	8000.478571	10.457152	-0.055978	4.816269
274.047060	8000.427360	10.462157	-0.055979	4.816254
274.055655	8000.591998	10.467162	-0.055980	4.816302
274.049493	8000.526725	10.472167	-0.055979	4.816283
274.099141	8000.496640	10.477171	-0.055988	4.816274
274.281000	8000.514872	10.482176	-0.056022	4.816278
274.420783	8000.413784	10.487181	-0.056048	4.816248
274.167381	8000.499989	10.492186	-0.056001	4.816274
274.128027	8000.516361	10.497191	-0.055993	4.816279
274.268611	8000.388585	10.502195	-0.056019	4.816241
274.265245	8000.504941	10.507200	-0.056019	4.816275
274.130000	8000.380727	10.512205	-0.055993	4.816240
274.192028	8000.421361	10.517210	-0.056005	4.816251
274.189040	8000.527043	10.522215	-0.056004	4.816282
274.339055	8000.377007	10.527219	-0.056032	4.816237
274.177397	8000.523615	10.532224	-0.056002	4.816281
274.514770	8000.429300	10.537229	-0.056065	4.816252
274.324809	8000.601034	10.542234	-0.056029	4.816303
274.168102	8000.493520	10.547239	-0.056000	4.816272
274.355058	8000.552433	10.552243	-0.056035	4.816289
274.379614	8000.603072	10.557248	-0.056039	4.816303
274.482923	8000.406261	10.562253	-0.056058	4.816245
274.330281	8000.514581	10.567258	-0.056030	4.816278
274.260139	8000.517580	10.572263	-0.056017	4.816279
274.466021	8000.551200	10.577267	-0.056055	4.816288
274.493858	8000.502563	10.582272	-0.056060	4.816273
274.809402	8000.380083	10.587277	-0.056119	4.816236
274.583192	8000.496687	10.592282	-0.056077	4.816271
274.486779	8000.505619	10.597287	-0.056059	4.816274
274.587574	8000.443347	10.602291	-0.056077	4.816256
274.394775	8000.512489	10.607296	-0.056041	4.816277
274.397217	8000.421737	10.612301	-0.056042	4.816250
274.359379	8000.506496	10.617306	-0.056035	4.816275
274.478827	8000.511851	10.622311	-0.056057	4.816276
274.528344	8000.496717	10.627315	-0.056066	4.816271
274.356739	8000.543812	10.632320	-0.056034	4.816286
274.519650	8000.616177	10.637325	-0.056064	4.816306
274.555368	8000.434167	10.642330	-0.056071	4.816253
274.523253	8000.463487	10.647335	-0.056065	4.816262
274.627378	8000.280578	10.652339	-0.056084	4.816208
274.573655	8000.525267	10.657344	-0.056074	4.816280
274.416409	8000.414540	10.662349	-0.056045	4.816248
274.320468	8000.520680	10.667354	-0.056027	4.816280
274.419313	8000.603636	10.672359	-0.056045	4.816303
274.610277	8000.430840	10.677363	-0.056081	4.816252
274.526974	8000.593819	10.682368	-0.056065	4.816300
274.701699	8000.531813	10.687373	-0.056097	4.816281
274.648402	8000.520162	10.692378	-0.056087	4.816278
274.415197	8000.442242	10.697383	-0.056044	4.816256
274.582995	8000.420700	10.702387	-0.056075	4.816249
274.500976	8000.606133	10.707392	-0.056060	4.816304
274.390786	8000.411874	10.712397	-0.056039	4.816247
274.292042	8000.547871	10.717402	-0.056021	4.816288
274.396201	8000.512362	10.722407	-0.056040	4.816277
274.338626	8000.510247	10.727411	-0.056029	4.816276
274.266617	8000.492917	10.732416	-0.056016	4.816272
274.455145	8000.521952	10.737421	-0.056051	4.816279
274.427651	8000.510767	10.742426	-0.056046	4.816276
274.464486	8000.518903	10.747431	-0.056052	4.816278
274.537074	8000.424077	10.752435	-0.056066	4.816250
274.497284	8000.565411	10.757440	-0.056058	4.816292
274.590586	8000.420758	10.762445	-0.056076	4.816249
274.509026	8000.400051	10.767450	-0.056060	4.816243
274.710372	8000.524380	10.772455	-0.056098	4.816279
274.834860	8000.421946	10.777459	-0.056121	4.816248
274.300128	8000.556475	10.782464	-0.056021	4.816290
274.387289	8000.497160	10.787469	-0.056038	4.816272
274.533289	8000.498723	10.792474	-0.056065	4.816272
274.479464	8000.495608	10.797479	-0.056055	4.816271
274.681045	8000.410589	10.802483	-0.056092	4.816246
274.456119	8000.534693	10.807488	-0.056050	4.816283
274.542891	8000.421966	10.812493	-0.056066	4.816250
274.572738	8000.510084	10.817498	-0.056072	4.816275
274.751633	8000.521855	10.822503	-0.056105	4.816278
274.509428	8000.515336	10.827507	-0.056060	4.816277
274.535065	8000.601242	10.832512	-0.056065	4.816302
274.793058	8000.394408	10.837517	-0.056112	4.816240
274.743126	8000.536628	10.842522	-0.056103	4.816282
274.528143	8000.611778	10.847527	-0.056063	4.816305
274.689253	8000.435238	10.852531	-0.056093	4.816253
274.823094	8000.519895	10.857536	-0.056118	4.816277
274.786555	8000.525637	10.862541	-0.056111	4.816279
274.768691	8000.517830	10.867546	-0.056107	4.816276
274.736040	8000.572777	10.872551	-0.056101	4.816293
274.750127	8000.388239	10.877555	-0.056104	4.816239
274.670578	8000.519242	10.882560	-0.056089	4.816277
274.584602	8000.525159	10.887565	-0.056073	4.816280
274.537132	8000.585178	10.892570	-0.056064	4.816297
274.624259	8000.542952	10.897575	-0.056080	4.816285
274.524201	8000.433258	10.902579	-0.056061	4.816253
274.627111	8000.560080	10.907584	-0.056081	4.816290
274.655202	8000.259372	10.912589	-0.056086	4.816202
274.505894	8000.507675	10.917594	-0.056058	4.816275
274.551856	8000.445480	10.922599	-0.056066	4.816256
274.735956	8000.362281	10.927603	-0.056100	4.816231
274.751699	8000.475780	10.932608	-0.056103	4.816264
274.859230	8000.390130	10.937613	-0.056123	4.816239
274.869732	8000.324090	10.942618	-0.056125	4.816219
274.580721	8000.396835	10.947623	-0.056071	4.816242
274.567598	8000.359207	10.952627	-0.056069	4.816231
274.690639	8000.430851	10.957632	-0.056092	4.816251
274.718921	8000.419606	10.962637	-0.056097	4.816248
274.654131	8000.510287	10.967642	-0.056085	4.816275
274.684843	8000.538606	10.972647	-0.056090	4.816283
274.789728	8000.400570	10.977651	-0.056110	4.816242
274.612375	8000.518057	10.982656	-0.056077	4.816277
274.850927	8000.386709	10.987661	-0.056121	4.816238
274.801455	8000.479803	10.992666	-0.056112	4.816265
274.685472	8000.383707	10.997671	-0.056090	4.816238
274.598205	8000.466505	11.002675	-0.056074	4.816262
274.436076	8000.575722	11.007680	-0.056044	4.816295
274.817123	8000.421313	11.012685	-0.056114	4.816248
274.802297	8000.406085	11.017690	-0.056112	4.816244
274.738039	8000.524547	11.022695	-0.056100	4.816279
274.923812	8000.397586	11.027699	-0.056134	4.816241
274.497751	8000.427266	11.032704	-0.056055	4.816251
274.581754	8000.514227	11.037709	-0.056070	4.816276
274.627046	8000.516106	11.042714	-0.056079	4.816277
274.576709	8000.504509	11.047719	-0.056069	4.816274
274.661026	8000.426985	11.052723	-0.056085	4.816251
274.609297	8000.528583	11.057728	-0.056075	4.816281
274.773233	8000.398023	11.062733	-0.056106	4.816242
274.623297	8000.496779	11.067738	-0.056078	4.816271
274.560329	8000.411253	11.072743	-0.056066	4.816246
274.880682	8000.434124	11.077747	-0.056125	4.816251
274.695391	8000.409408	11.082752	-0.056091	4.816245
274.533033	8000.374425	11.087757	-0.056060	4.816236
274.968394	8000.532889	11.092762	-0.056142	4.816280
274.850248	8000.418594	11.097767	-0.056119	4.816247
274.825101	8000.515333	11.102771	-0.056115	4.816276
274.815844	8000.495932	11.107776	-0.056113	4.816270
274.899184	8000.278466	11.112781	-0.056128	4.816206
274.860389	8000.389911	11.117786	-0.056121	4.816239
274.619606	8000.381282	11.122791	-0.056076	4.816237
274.748652	8000.301362	11.127795	-0.056100	4.816213
274.609565	8000.496444	11.132800	-0.056074	4.816271
274.791356	8000.414272	11.137805	-0.056108	4.816246
274.959084	8000.472839	11.142810	-0.056139	4.816262
274.946410	8000.441627	11.147815	-0.056137	4.816253
274.911555	8000.363018	11.152819	-0.056130	4.816231
274.786887	8000.435528	11.157824	-0.056107	4.816252
274.922396	8000.410198	11.162829	-0.056132	4.816244
274.923509	8000.436915	11.167834	-0.056132	4.816252
274.836333	8000.501557	11.172839	-0.056116	4.816271
274.988559	8000.310970	11.177843	-0.056144	4.816215
274.777011	8000.422498	11.182848	-0.056105	4.816249
274.767699	8000.516318	11.187853	-0.056103	4.816276
274.803993	8000.364226	11.192858	-0.056110	4.816232
274.810365	8000.527757	11.197863	-0.056111	4.816279
274.779791	8000.513313	11.202867	-0.056105	4.816275
274.875444	8000.520375	11.207872	-0.056123	4.816277
274.912738	8000.404616	11.212877	-0.056130	4.816243
274.808978	8000.311945	11.217882	-0.056110	4.816216
274.633819	8000.476469	11.222887	-0.056077	4.816265
274.842952	8000.531511	11.227891	-0.056116	4.816280
274.774577	8000.538813	11.232896	-0.056104	4.816283
274.782385	8000.479133	11.237901	-0.056105	4.816265
274.709533	8000.432949	11.242906	-0.056091	4.816252
274.779701	8000.498297	11.247911	-0.056104	4.816271
274.916352	8000.536008	11.252915	-0.056130	4.816281
274.824201	8000.435000	11.257920	-0.056112	4.816252
274.848465	8000.434364	11.262925	-0.056117	4.816252
274.805167	8000.522230	11.267930	-0.056109	4.816278
274.784556	8000.513305	11.272935	-0.056105	4.816275
275.009006	8000.406269	11.277939	-0.056147	4.816243
274.949430	8000.526953	11.282944	-0.056135	4.816278
274.931449	8000.417672	11.287949	-0.056132	4.816246
274.869215	8000.519081	11.292954	-0.056120	4.816276
274.950665	8000.437232	11.297959	-0.056135	4.816252
274.874150	8000.434775	11.302963	-0.056121	4.816252
274.684092	8000.529602	11.307968	-0.056086	4.816281
274.931049	8000.459288	11.312973	-0.056132	4.816259
274.733165	8000.514453	11.317978	-0.056095	4.816276
274.844596	8000.400034	11.322983	-0.056115	4.816242
274.837344	8000.376398	11.327987	-0.056114	4.816235
274.909885	8000.489855	11.332992	-0.056127	4.816268
274.899636	8000.424507	11.337997	-0.056125	4.816249
274.793714	8000.530468	11.343002	-0.056106	4.816280
274.745180	8000.392864	11.348007	-0.056096	4.816240
274.974343	8000.443995	11.353011	-0.056139	4.816254
274.893999	8000.442537	11.358016	-0.056124	4.816254
274.765502	8000.388939	11.363021	-0.056100	4.816239
275.048016	8000.384423	11.368026	-0.056153	4.816236
274.920033	8000.498530	11.373031	-0.056129	4.816270
275.076259	8000.355013	11.378035	-0.056158	4.816227
274.841745	8000.471467	11.383040	-0.056114	4.816263
274.943135	8000.456203	11.388045	-0.056133	4.816258
274.784891	8000.518492	11.393050	-0.056103	4.816277
274.955380	8000.514089	11.398055	-0.056135	4.816275
275.157669	8000.526283	11.403059	-0.056173	4.816277
274.911392	8000.605141	11.408064	-0.056127	4.816301
274.861642	8000.440811	11.413069	-0.056117	4.816254
274.799003	8000.433264	11.418074	-0.056106	4.816252
274.786566	8000.499256	11.423079	-0.056103	4.816271
274.916529	8000.531506	11.428083	-0.056127	4.816280
274.850040	8000.523889	11.433088	-0.056115	4.816278
274.977226	8000.503750	11.438093	-0.056138	4.816271
274.920901	8000.421548	11.443098	-0.056128	4.816248
274.852122	8000.566632	11.448103	-0.056115	4.816291
275.044766	8000.407750	11.453107	-0.056151	4.816243
274.906184	8000.548369	11.458112	-0.056125	4.816285
274.987080	8000.407763	11.463117	-0.056140	4.816243
274.869231	8000.538075	11.468122	-0.056118	4.816282
274.798255	8000.517559	11.473127	-0.056105	4.816276
274.876004	8000.407872	11.478131	-0.056119	4.816244
275.003243	8000.522318	11.483136	-0.056143	4.816277
275.137604	8000.510854	11.488141	-0.056168	4.816273
275.161871	8000.516626	11.493146	-0.056172	4.816274
275.095827	8000.509017	11.498151	-0.056160	4.816272
275.236628	8000.521168	11.503155	-0.056186	4.816275
275.096257	8000.491922	11.508160	-0.056160	4.816267
275.027679	8000.467177	11.513165	-0.056147	4.816261
275.215657	8000.526110	11.518170	-0.056182	4.816277
275.068785	8000.527722	11.523175	-0.056154	4.816278
274.896495	8000.493626	11.528179	-0.056122	4.816269
274.883698	8000.512614	11.533184	-0.056120	4.816275
274.975298	8000.509990	11.538189	-0.056137	4.816273
274.869012	8000.510200	11.543194	-0.056117	4.816274
274.894986	8000.507458	11.548199	-0.056122	4.816273
275.184677	8000.413350	11.553203	-0.056175	4.816244
275.016497	8000.507504	11.558208	-0.056144	4.816272
275.085418	8000.464949	11.563213	-0.056157	4.816260
275.299532	8000.354521	11.568218	-0.056197	4.816226
275.157751	8000.533535	11.573223	-0.056170	4.816279
275.061022	8000.407878	11.578227	-0.056152	4.816243
275.047054	8000.514432	11.583232	-0.056150	4.816274
275.092061	8000.335793	11.588237	-0.056158	4.816222
274.953127	8000.427271	11.593242	-0.056132	4.816249
275.005702	8000.533959	11.598247	-0.056142	4.816280
275.063781	8000.348079	11.603251	-0.056152	4.816226
275.016375	8000.599295	11.608256	-0.056144	4.816299
275.145608	8000.480924	11.613261	-0.056167	4.816264
275.132683	8000.379212	11.618266	-0.056165	4.816234
275.085932	8000.465947	11.623271	-0.056156	4.816260
275.116007	8000.429099	11.628275	-0.056162	4.816249
275.191384	8000.525518	11.633280	-0.056176	4.816277
274.962632	8000.387862	11.638285	-0.056133	4.816238
274.840172	8000.503137	11.643290	-0.056110	4.816272
274.889902	8000.442077	11.648295	-0.056119	4.816254
275.190309	8000.535085	11.653299	-0.056175	4.816280
275.331779	8000.273807	11.658304	-0.056201	4.816202
275.068939	8000.361978	11.663309	-0.056152	4.816230
275.159892	8000.409544	11.668314	-0.056169	4.816243
275.124666	8000.414242	11.673319	-0.056163	4.816245
275.191533	8000.404762	11.678323	-0.056175	4.816242
275.049280	8000.494044	11.683328	-0.056149	4.816268
275.250599	8000.536128	11.688333	-0.056186	4.816280
275.317788	8000.502087	11.693338	-0.056198	4.816269
275.189639	8000.610851	11.698343	-0.056175	4.816302
275.172134	8000.515464	11.703347	-0.056171	4.816274
275.326003	8000.499011	11.708352	-0.056200	4.816268
275.051052	8000.514331	11.713357	-0.056148	4.816274
275.028083	8000.438072	11.718362	-0.056144	4.816252
275.037092	8000.409388	11.723367	-0.056146	4.816244
275.303873	8000.341569	11.728371	-0.056195	4.816222
275.276365	8000.409426	11.733376	-0.056190	4.816242
275.469971	8000.372329	11.738381	-0.056226	4.816231
275.336913	8000.529070	11.743386	-0.056201	4.816277
275.237883	8000.529410	11.748391	-0.056183	4.816278
275.540232	8000.397077	11.753395	-0.056239	4.816237
275.299714	8000.521969	11.758400	-0.056194	4.816275
275.192321	8000.524294	11.763405	-0.056174	4.816276
275.089471	8000.538451	11.768410	-0.056155	4.816281
275.235863	8000.517591	11.773415	-0.056182	4.816274
275.232316	8000.393616	11.778419	-0.056181	4.816238
275.200553	8000.419739	11.783424	-0.056175	4.816246
275.300651	8000.257049	11.788429	-0.056194	4.816198
275.370565	8000.424934	11.793434	-0.056207	4.816246
275.131376	8000.409924	11.798439	-0.056162	4.816243
275.322595	8000.448621	11.803443	-0.056198	4.816254
275.223760	8000.393422	11.808448	-0.056179	4.816238
275.165859	8000.379551	11.813453	-0.056168	4.816234
275.107128	8000.430822	11.818458	-0.056157	4.816250
275.404365	8000.396665	11.823463	-0.056213	4.816238
275.293509	8000.385042	11.828467	-0.056192	4.816235
275.309016	8000.438722	11.833472	-0.056195	4.816251
275.322902	8000.401582	11.838477	-0.056197	4.816240
275.235687	8000.476905	11.843482	-0.056181	4.816262
275.010943	8000.316891	11.848487	-0.056139	4.816217
275.095636	8000.528836	11.853491	-0.056155	4.816278
275.016246	8000.374652	11.858496	-0.056140	4.816234
275.034874	8000.517043	11.863501	-0.056143	4.816275
275.149441	8000.427247	11.868506	-0.056165	4.816248
275.263223	8000.509407	11.873511	-0.056186	4.816272
275.322702	8000.514748	11.878515	-0.056197	4.816273
275.162889	8000.486218	11.883520	-0.056167	4.816266
275.292829	8000.412721	11.888525	-0.056191	4.816243
275.441306	8000.432488	11.893530	-0.056219	4.816248
275.220900	8000.425294	11.898535	-0.056177	4.816247
275.234797	8000.392427	11.903539	-0.056180	4.816238
275.389884	8000.522331	11.908544	-0.056209	4.816275
275.205592	8000.518993	11.913549	-0.056175	4.816275
275.067851	8000.366960	11.918554	-0.056149	4.816231
275.180484	8000.515322	11.923559	-0.056170	4.816274
275.309304	8000.110687	11.928563	-0.056193	4.816155
275.249357	8000.381968	11.933568	-0.056182	4.816235
275.345412	8000.506533	11.938573	-0.056200	4.816271
275.407903	8000.414728	11.943578	-0.056212	4.816243
275.198092	8000.524152	11.948583	-0.056173	4.816276
275.460853	8000.332357	11.953587	-0.056221	4.816219
275.420906	8000.518552	11.958592	-0.056214	4.816274
275.300758	8000.370040	11.963597	-0.056191	4.816231
275.245605	8000.536733	11.968602	-0.056181	4.816280
275.358484	8000.420203	11.973607	-0.056202	4.816245
275.508540	8000.512632	11.978611	-0.056230	4.816271
275.251642	8000.422532	11.983616	-0.056182	4.816246
275.447138	8000.309632	11.988621	-0.056218	4.816212
275.484178	8000.468378	11.993626	-0.056225	4.816259
275.376680	8000.537994	11.998631	-0.056205	4.816280
275.351308	8000.392262	12.003635	-0.056200	4.816237
275.497701	8000.505988	12.008640	-0.056228	4.816270
275.464047	8000.533144	12.013645	-0.056221	4.816278
275.312130	8000.516506	12.018650	-0.056193	4.816274
275.347306	8000.339825	12.023655	-0.056199	4.816222
275.236567	8000.392292	12.028659	-0.056179	4.816238
275.319145	8000.527295	12.033664	-0.056194	4.816277
275.220800	8000.519102	12.038669	-0.056176	4.816275
275.497221	8000.391641	12.043674	-0.056227	4.816236
275.485342	8000.537755	12.048679	-0.056225	4.816279
275.334682	8000.416462	12.053683	-0.056197	4.816244
275.465379	8000.501064	12.058688	-0.056221	4.816268
275.467270	8000.402823	12.063693	-0.056221	4.816240
275.402937	8000.437970	12.068698	-0.056209	4.816250
275.288553	8000.521348	12.073703	-0.056188	4.816275
275.635345	8000.258438	12.078707	-0.056252	4.816197
275.523372	8000.468967	12.083712	-0.056231	4.816259
275.241912	8000.292973	12.088717	-0.056179	4.816209
275.432735	8000.542085	12.093722	-0.056214	4.816281
275.286113	8000.502044	12.098727	-0.056187	4.816270
275.352459	8000.259702	12.103731	-0.056199	4.816198
275.269283	8000.528430	12.108736	-0.056184	4.816277
275.455700	8000.344868	12.113741	-0.056218	4.816223
275.363179	8000.424368	12.118746	-0.056201	4.816246
275.334293	8000.518903	12.123751	-0.056196	4.816274
275.515736	8000.371568	12.128755	-0.056229	4.816230
275.365860	8000.483144	12.133760	-0.056201	4.816264
275.446479	8000.369235	12.138765	-0.056216	4.816230
275.353142	8000.300250	12.143770	-0.056199	4.816210
275.500545	8000.417197	12.148775	-0.056226	4.816244
275.376314	8000.215206	12.153779	-0.056203	4.816185
275.467724	8000.401637	12.158784	-0.056220	4.816239
275.435930	8000.376488	12.163789	-0.056214	4.816232
275.433855	8000.423442	12.168794	-0.056213	4.816246
275.322615	8000.506876	12.173799	-0.056193	4.816271
275.440164	8000.395771	12.178803	-0.056214	4.816238
275.388312	8000.435417	12.183808	-0.056205	4.816250
275.467416	8000.350321	12.188813	-0.056219	4.816224
275.654810	8000.403903	12.193818	-0.056254	4.816239
275.603140	8000.413644	12.198823	-0.056245	4.816242
275.670950	8000.374273	12.203827	-0.056257	4.816230
275.401156	8000.315985	12.208832	-0.056207	4.816215
275.514739	8000.469706	12.213837	-0.056228	4.816259
275.639945	8000.349126	12.218842	-0.056251	4.816223
275.559568	8000.312418	12.223847	-0.056236	4.816213
275.751745	8000.369291	12.228851	-0.056272	4.816228
275.615816	8000.515300	12.233856	-0.056246	4.816272
275.591956	8000.468932	12.238861	-0.056242	4.816258
275.462752	8000.415319	12.243866	-0.056218	4.816243
275.340674	8000.496421	12.248871	-0.056195	4.816268
275.449474	8000.407589	12.253875	-0.056215	4.816241
275.393969	8000.525143	12.258880	-0.056205	4.816276
275.306465	8000.398583	12.263885	-0.056188	4.816239
275.392811	8000.422567	12.268890	-0.056204	4.816246
275.312910	8000.519385	12.273895	-0.056190	4.816275
275.449306	8000.412894	12.278899	-0.056215	4.816243
275.662440	8000.402853	12.283904	-0.056254	4.816239
275.382542	8000.506738	12.288909	-0.056202	4.816271
275.388209	8000.414974	12.293914	-0.056203	4.816244
275.367074	8000.503241	12.298919	-0.056199	4.816270
275.492314	8000.425387	12.303923	-0.056222	4.816246
275.484629	8000.473308	12.308928	-0.056221	4.816260
275.377340	8000.408342	12.313933	-0.056201	4.816242
275.454849	8000.187565	12.318938	-0.056215	4.816177
275.510771	8000.468419	12.323943	-0.056226	4.816259
275.723040	8000.495748	12.328947	-0.056265	4.816266
275.518861	8000.418350	12.333952	-0.056227	4.816244
275.397108	8000.533638	12.338957	-0.056204	4.816278
275.568227	8000.514293	12.343962	-0.056236	4.816272
275.484897	8000.535211	12.348967	-0.056221	4.816278
275.540543	8000.325787	12.353971	-0.056231	4.816217
275.482089	8000.432606	12.358976	-0.056220	4.816248
275.538290	8000.394094	12.363981	-0.056230	4.816237
275.745810	8000.333749	12.368986	-0.056269	4.816218
275.682599	8000.369985	12.373991	-0.056257	4.816229
275.706481	8000.239029	12.378995	-0.056261	4.816191
275.626617	8000.347597	12.384000	-0.056246	4.816223
275.521686	8000.492029	12.389005	-0.056227	4.816266
275.695334	8000.303964	12.394010	-0.056259	4.816210
275.502794	8000.501288	12.399015	-0.056223	4.816268
275.495943	8000.408229	12.404019	-0.056222	4.816241
275.491510	8000.537387	12.409024	-0.056221	4.816279
275.648957	8000.359710	12.414029	-0.056250	4.816226
275.474523	8000.421708	12.419034	-0.056218	4.816245
275.356681	8000.407822	12.424039	-0.056196	4.816242
275.473369	8000.235819	12.429043	-0.056217	4.816191
275.592028	8000.511399	12.434048	-0.056239	4.816271
275.451412	8000.252499	12.439053	-0.056213	4.816196
275.523302	8000.387308	12.444058	-0.056226	4.816235
275.513615	8000.483258	12.449063	-0.056224	4.816263
275.449538	8000.295170	12.454067	-0.056212	4.816208
275.460779	8000.317797	12.459072	-0.056214	4.816215
275.715756	8000.321330	12.464077	-0.056262	4.816215
275.631023	8000.294157	12.469082	-0.056246	4.816207
275.552184	8000.379244	12.474087	-0.056231	4.816232
275.682492	8000.417909	12.479091	-0.056255	4.816243
275.648610	8000.413018	12.484096	-0.056249	4.816242
275.731820	8000.539488	12.489101	-0.056265	4.816278
275.633126	8000.271731	12.494106	-0.056246	4.816201
275.571301	8000.413737	12.499111	-0.056235	4.816242
275.594819	8000.401338	12.504115	-0.056239	4.816239
275.482666	8000.506118	12.509120	-0.056218	4.816270
275.554308	8000.531974	12.514125	-0.056231	4.816277
275.627780	8000.461729	12.519130	-0.056245	4.816256
275.523272	8000.515377	12.524135	-0.056225	4.816272
275.654193	8000.356447	12.529139	-0.056249	4.816225
275.643746	8000.422477	12.534144	-0.056248	4.816245
275.537352	8000.431229	12.539149	-0.056228	4.816248
275.703010	8000.437420	12.544154	-0.056258	4.816249
275.761351	8000.378652	12.549159	-0.056269	4.816231
275.774867	8000.365004	12.554163	-0.056272	4.816227
275.780392	8000.463366	12.559168	-0.056273	4.816256
275.619228	8000.379268	12.564173	-0.056243	4.816232
275.740767	8000.415638	12.569178	-0.056265	4.816242
275.565562	8000.488303	12.574183	-0.056232	4.816264
275.634914	8000.405167	12.579187	-0.056245	4.816240
275.549174	8000.411088	12.584192	-0.056229	4.816242
275.525261	8000.372196	12.589197	-0.056225	4.816231
275.522168	8000.358248	12.594202	-0.056224	4.816227
275.597601	8000.423692	12.599207	-0.056238	4.816245
275.811753	8000.272676	12.604211	-0.056278	4.816200
275.718371	8000.403431	12.609216	-0.056260	4.816239
275.756908	8000.321874	12.614221	-0.056267	4.816215
275.800238	8000.180588	12.619226	-0.056275	4.816173
275.748277	8000.348408	12.624231	-0.056266	4.816222
275.699973	8000.392390	12.629235	-0.056257	4.816236
275.705573	8000.387144	12.634240	-0.056258	4.816234
275.610270	8000.243353	12.639245	-0.056240	4.816192
275.737742	8000.336441	12.644250	-0.056263	4.816219
275.792008	8000.364119	12.649255	-0.056274	4.816227
275.817570	8000.381664	12.654259	-0.056278	4.816232
275.634827	8000.324948	12.659264	-0.056244	4.816216
275.514526	8000.354812	12.664269	-0.056222	4.816226
275.582684	8000.380604	12.669274	-0.056234	4.816233
275.354719	8000.399977	12.674279	-0.056192	4.816240
275.397331	8000.396468	12.679283	-0.056200	4.816238
275.676395	8000.419662	12.684288	-0.056252	4.816244
275.571621	8000.414558	12.689293	-0.056232	4.816243
275.594009	8000.276098	12.694298	-0.056236	4.816202
275.554035	8000.320231	12.699303	-0.056228	4.816215
275.747263	8000.368578	12.704307	-0.056264	4.816228
275.562533	8000.378050	12.709312	-0.056230	4.816232
275.518621	8000.229848	12.714317	-0.056222	4.816189
275.697424	8000.432814	12.719322	-0.056255	4.816247
275.706969	8000.505613	12.724327	-0.056257	4.816269
275.655840	8000.173561	12.729331	-0.056247	4.816172
275.539841	8000.471603	12.734336	-0.056225	4.816260
275.479829	8000.379720	12.739341	-0.056214	4.816233
275.589730	8000.403062	12.744346	-0.056235	4.816239
275.634060	8000.372881	12.749351	-0.056243	4.816230
275.615544	8000.363995	12.754355	-0.056239	4.816228
275.591539	8000.516298	12.759360	-0.056235	4.816272
275.652960	8000.528083	12.764365	-0.056246	4.816276
275.801197	8000.421805	12.769370	-0.056274	4.816244
275.571215	8000.515911	12.774375	-0.056231	4.816272
275.617801	8000.380024	12.779379	-0.056239	4.816232
275.563771	8000.413221	12.784384	-0.056229	4.816242
275.815425	8000.393195	12.789389	-0.056276	4.816235
275.729213	8000.346769	12.794394	-0.056260	4.816222
275.629855	8000.478484	12.799399	-0.056241	4.816261
275.775154	8000.380698	12.804403	-0.056268	4.816232
276.003340	8000.336749	12.809408	-0.056311	4.816218
275.779413	8000.422419	12.814413	-0.056269	4.816244
275.950755	8000.294128	12.819418	-0.056301	4.816206
275.835383	8000.382828	12.824423	-0.056279	4.816232
275.921545	8000.279701	12.829427	-0.056295	4.816202
275.791231	8000.505922	12.834432	-0.056271	4.816268
275.566801	8000.398249	12.839437	-0.056229	4.816238
275.716790	8000.427656	12.844442	-0.056257	4.816246
275.404565	8000.456188	12.849447	-0.056199	4.816256
275.739334	8000.417369	12.854451	-0.056261	4.816243
275.772923	8000.461763	12.859456	-0.056267	4.816256
275.585660	8000.521393	12.864461	-0.056232	4.816274
275.624601	8000.384300	12.869466	-0.056239	4.816234
275.795843	8000.501679	12.874471	-0.056271	4.816267
275.786028	8000.447020	12.879475	-0.056269	4.816251
275.684948	8000.382166	12.884480	-0.056250	4.816233
275.861923	8000.508194	12.889485	-0.056283	4.816269
276.019029	8000.278171	12.894490	-0.056312	4.816201
275.871799	8000.509428	12.899495	-0.056285	4.816269
275.845222	8000.430966	12.904499	-0.056280	4.816246
275.928727	8000.450627	12.909504	-0.056295	4.816251
275.766819	8000.459444	12.914509	-0.056265	4.816255
275.735878	8000.459946	12.919514	-0.056259	4.816255
275.763959	8000.521331	12.924519	-0.056265	4.816273
275.649043	8000.457295	12.929523	-0.056243	4.816255
275.754711	8000.529696	12.934528	-0.056263	4.816276
275.771790	8000.523589	12.939533	-0.056266	4.816274
275.824906	8000.438022	12.944538	-0.056276	4.816248
275.619684	8000.516554	12.949543	-0.056237	4.816272
275.823068	8000.395250	12.954547	-0.056275	4.816236
275.725854	8000.356102	12.959552	-0.056257	4.816225
275.633063	8000.430256	12.964557	-0.056240	4.816247
275.795723	8000.297535	12.969562	-0.056270	4.816207
275.736641	8000.531452	12.974567	-0.056259	4.816276
275.617219	8000.392565	12.979571	-0.056236	4.816236
275.621364	8000.399042	12.984576	-0.056237	4.816238
275.711131	8000.523494	12.989581	-0.056254	4.816274
275.882379	8000.406950	12.994586	-0.056286	4.816239
275.713708	8000.476529	12.999591	-0.056254	4.816260
275.845651	8000.235371	13.004595	-0.056279	4.816189
275.757632	8000.360882	13.009600	-0.056262	4.816226
275.646755	8000.490253	13.014605	-0.056242	4.816265
275.927655	8000.250718	13.019610	-0.056294	4.816193
275.966642	8000.519521	13.024615	-0.056301	4.816271
275.823470	8000.197552	13.029619	-0.056274	4.816178
275.723730	8000.415779	13.034624	-0.056256	4.816242
275.919062	8000.372304	13.039629	-0.056292	4.816229
276.009565	8000.256438	13.044634	-0.056309	4.816194
275.796233	8000.496112	13.049639	-0.056269	4.816266
275.862242	8000.334941	13.054643	-0.056281	4.816218
275.921243	8000.424656	13.059648	-0.056292	4.816244
275.799097	8000.450214	13.064653	-0.056269	4.816252
276.015460	8000.273601	13.069658	-0.056309	4.816199
275.923811	8000.418274	13.074663	-0.056292	4.816242
275.903855	8000.431792	13.079667	-0.056288	4.816246
275.949211	8000.475331	13.084672	-0.056297	4.816259
275.773388	8000.470011	13.089677	-0.056264	4.816258
275.893418	8000.405948	13.094682	-0.056286	4.816239
275.951135	8000.518072	13.099687	-0.056297	4.816271
275.925468	8000.404378	13.104691	-0.056292	4.816238
276.047138	8000.425797	13.109696	-0.056315	4.816244
276.025527	8000.402969	13.114701	-0.056311	4.816237
276.012344	8000.292705	13.119706	-0.056308	4.816205
276.075555	8000.362202	13.124711	-0.056320	4.816225
276.033163	8000.460767	13.129715	-0.056312	4.816254
275.878095	8000.393869	13.134720	-0.056283	4.816235
276.009938	8000.525491	13.139725	-0.056307	4.816273
276.006799	8000.404726	13.144730	-0.056307	4.816238
275.926613	8000.440656	13.149735	-0.056292	4.816249
275.962327	8000.252233	13.154739	-0.056298	4.816193
275.989922	8000.407606	13.159744	-0.056303	4.816239
275.891185	8000.451745	13.164749	-0.056285	4.816252
276.037098	8000.380673	13.169754	-0.056312	4.816231
275.923919	8000.441642	13.174759	-0.056291	4.816249
276.091882	8000.373105	13.179763	-0.056322	4.816228
275.779163	8000.295882	13.184768	-0.056264	4.816207
275.751954	8000.517557	13.189773	-0.056259	4.816272
275.939460	8000.411988	13.194778	-0.056294	4.816240
275.802711	8000.320854	13.199783	-0.056268	4.816214
275.980929	8000.466132	13.204787	-0.056301	4.816256
276.150400	8000.326056	13.209792	-0.056333	4.816214
275.922211	8000.514192	13.214797	-0.056290	4.816270
275.883358	8000.379965	13.219802	-0.056283	4.816231
276.010901	8000.527531	13.224807	-0.056306	4.816274
275.938461	8000.438627	13.229811	-0.056293	4.816248
275.904504	8000.387804	13.234816	-0.056286	4.816233
275.830702	8000.411031	13.239821	-0.056273	4.816241
276.061601	8000.310519	13.244826	-0.056316	4.816210
275.964511	8000.430526	13.249831	-0.056297	4.816246
275.730568	8000.271412	13.254835	-0.056254	4.816200
275.900115	8000.453916	13.259840	-0.056285	4.816253
275.734605	8000.234087	13.264845	-0.056254	4.816189
275.794766	8000.344117	13.269850	-0.056266	4.816221
275.821717	8000.428980	13.274855	-0.056271	4.816246
276.032096	8000.285372	13.279859	-0.056310	4.816203
275.947607	8000.495331	13.284864	-0.056294	4.816265
275.867510	8000.423379	13.289869	-0.056279	4.816244
276.187990	8000.357599	13.294874	-0.056338	4.816223
275.736137	8000.368653	13.299879	-0.056254	4.816229
275.803958	8000.378417	13.304883	-0.056267	4.816231
276.033862	8000.419950	13.309888	-0.056310	4.816242
276.010387	8000.375725	13.314893	-0.056305	4.816229
275.913244	8000.413484	13.319898	-0.056287	4.816241
275.766608	8000.430054	13.324903	-0.056260	4.816246
275.980397	8000.427502	13.329907	-0.056299	4.816245
276.174160	8000.390408	13.334912	-0.056335	4.816233
275.947014	8000.415136	13.339917	-0.056293	4.816241
276.164500	8000.276997	13.344922	-0.056333	4.816200
276.002548	8000.522941	13.349927	-0.056303	4.816272
275.968160	8000.325774	13.354931	-0.056297	4.816215
276.123901	8000.388398	13.359936	-0.056326	4.816232
276.256716	8000.414291	13.364941	-0.056350	4.816239
276.191555	8000.296679	13.369946	-0.056338	4.816205
276.042719	8000.410410	13.374951	-0.056310	4.816239
276.230322	8000.277071	13.379955	-0.056345	4.816199
276.320174	8000.287234	13.384960	-0.056362	4.816202
276.200472	8000.340607	13.389965	-0.056339	4.816218
276.153244	8000.219047	13.394970	-0.056330	4.816183
276.090843	8000.443291	13.399975	-0.056319	4.816249
275.945793	8000.388324	13.404979	-0.056292	4.816233
275.805710	8000.433852	13.409984	-0.056266	4.816247
275.969235	8000.532934	13.414989	-0.056296	4.816276
275.940888	8000.271788	13.419994	-0.056291	4.816199
275.906139	8000.552075	13.424999	-0.056284	4.816281
275.918501	8000.433727	13.430003	-0.056286	4.816247
275.956274	8000.345747	13.435008	-0.056293	4.816221
276.033623	8000.327912	13.440013	-0.056308	4.816215
276.150589	8000.353518	13.445018	-0.056329	4.816222
276.086166	8000.481594	13.450023	-0.056317	4.816260
276.080827	8000.480422	13.455027	-0.056316	4.816260
275.931665	8000.380518	13.460032	-0.056288	4.816231
276.083653	8000.527459	13.465037	-0.056317	4.816273
275.992437	8000.286538	13.470042	-0.056300	4.816203
275.908317	8000.338419	13.475047	-0.056284	4.816219
276.059069	8000.232186	13.480051	-0.056312	4.816187
276.100417	8000.380330	13.485056	-0.056319	4.816230
276.033599	8000.406888	13.490061	-0.056307	4.816238
276.162274	8000.253257	13.495066	-0.056331	4.816193
276.244484	8000.148991	13.500071	-0.056346	4.816162
276.120714	8000.204427	13.505075	-0.056323	4.816179
275.893580	8000.323152	13.510080	-0.056281	4.816215
275.912716	8000.327763	13.515085	-0.056284	4.816216
276.124428	8000.327310	13.520090	-0.056323	4.816215
276.099061	8000.449682	13.525095	-0.056319	4.816251
276.242818	8000.433047	13.530099	-0.056345	4.816245
276.271850	8000.439974	13.535104	-0.056351	4.816247
276.046586	8000.398511	13.540109	-0.056309	4.816236
276.094639	8000.270127	13.545114	-0.056318	4.816198
276.146709	8000.408852	13.550119	-0.056327	4.816238
276.066152	8000.415935	13.555123	-0.056312	4.816241
276.184911	8000.378553	13.560128	-0.056334	4.816229
276.192203	8000.398973	13.565133	-0.056335	4.816235
276.187466	8000.367904	13.570138	-0.056335	4.816226
276.113896	8000.369772	13.575143	-0.056321	4.816227
276.087136	8000.336170	13.580147	-0.056316	4.816217
276.082145	8000.265575	13.585152	-0.056315	4.816197
275.975681	8000.451638	13.590157	-0.056295	4.816252
276.177418	8000.284374	13.595162	-0.056332	4.816202
276.097472	8000.394010	13.600167	-0.056317	4.816234
276.037614	8000.415352	13.605171	-0.056306	4.816241
276.014331	8000.406380	13.610176	-0.056302	4.816238
276.046340	8000.273434	13.615181	-0.056308	4.816199
276.088066	8000.313702	13.620186	-0.056315	4.816211
276.012176	8000.304847	13.625191	-0.056301	4.816209
276.237196	8000.319588	13.630195	-0.056343	4.816212
276.283225	8000.335368	13.635200	-0.056351	4.816216
276.181677	8000.321776	13.640205	-0.056332	4.816213
276.368681	8000.232220	13.645210	-0.056367	4.816186
276.049372	8000.338598	13.650215	-0.056308	4.816218
276.244607	8000.412618	13.655219	-0.056344	4.816239
276.176392	8000.403901	13.660224	-0.056331	4.816237
276.113597	8000.403828	13.665229	-0.056319	4.816237
276.068513	8000.260943	13.670234	-0.056311	4.816196
275.970166	8000.440744	13.675239	-0.056293	4.816249
276.145906	8000.515480	13.680243	-0.056325	4.816270
276.263594	8000.402240	13.685248	-0.056347	4.816236
276.070736	8000.413701	13.690253	-0.056311	4.816240
276.178678	8000.225516	13.695258	-0.056331	4.816185
276.197082	8000.544150	13.700263	-0.056335	4.816278
276.111724	8000.448603	13.705267	-0.056319	4.816250
276.135901	8000.382808	13.710272	-0.056323	4.816231
276.126831	8000.414682	13.715277	-0.056321	4.816240
276.462636	8000.244500	13.720282	-0.056384	4.816189
276.140075	8000.441612	13.725287	-0.056324	4.816248
276.344275	8000.184668	13.730291	-0.056361	4.816172
276.237661	8000.376069	13.735296	-0.056342	4.816228
276.216293	8000.388494	13.740301	-0.056338	4.816232
276.175674	8000.182670	13.745306	-0.056330	4.816172
276.376242	8000.379622	13.750311	-0.056367	4.816229
276.203761	8000.302796	13.755315	-0.056335	4.816207
276.129173	8000.281146	13.760320	-0.056321	4.816201
276.109909	8000.381197	13.765325	-0.056317	4.816231
276.298837	8000.168840	13.770330	-0.056352	4.816168
276.168493	8000.508285	13.775335	-0.056328	4.816267
275.977924	8000.262364	13.780339	-0.056293	4.816197
276.147119	8000.298528	13.785344	-0.056324	4.816206
276.040747	8000.487797	13.790349	-0.056304	4.816262
276.173745	8000.394060	13.795354	-0.056329	4.816234
276.190068	8000.506505	13.800359	-0.056332	4.816267
276.347556	8000.332031	13.805363	-0.056361	4.816215
276.379585	8000.447964	13.810368	-0.056367	4.816249
276.164348	8000.438726	13.815373	-0.056327	4.816247
276.262661	8000.389225	13.820378	-0.056345	4.816232
276.132948	8000.436009	13.825383	-0.056321	4.816246
276.144982	8000.374267	13.830387	-0.056323	4.816228
276.238689	8000.420817	13.835392	-0.056340	4.816242
276.143474	8000.521632	13.840397	-0.056323	4.816271
276.171314	8000.322384	13.845402	-0.056328	4.816213
276.147817	8000.396723	13.850407	-0.056323	4.816235
276.316118	8000.374123	13.855411	-0.056355	4.816227
276.213660	8000.365855	13.860416	-0.056335	4.816226
276.271343	8000.293189	13.865421	-0.056346	4.816204
276.405487	8000.388536	13.870426	-0.056371	4.816231
276.216929	8000.391530	13.875431	-0.056336	4.816233
276.288930	8000.419529	13.880435	-0.056349	4.816241
276.225535	8000.298743	13.885440	-0.056337	4.816206
276.170910	8000.412041	13.890445	-0.056327	4.816239
276.110101	8000.293440	13.895450	-0.056316	4.816205
276.031431	8000.517390	13.900455	-0.056301	4.816271
276.187972	8000.299106	13.905459	-0.056330	4.816206
276.298008	8000.411107	13.910464	-0.056350	4.816238
276.122106	8000.488033	13.915469	-0.056318	4.816262
276.378928	8000.256607	13.920474	-0.056365	4.816193
276.415703	8000.371557	13.925479	-0.056372	4.816226
276.337607	8000.116989	13.930483	-0.056357	4.816152
276.395205	8000.375446	13.935488	-0.056368	4.816227
276.412328	8000.371476	13.940493	-0.056371	4.816226
276.419998	8000.336359	13.945498	-0.056373	4.816216
276.227151	8000.419387	13.950503	-0.056337	4.816241
276.236883	8000.356535	13.955507	-0.056338	4.816223
276.508439	8000.294143	13.960512	-0.056389	4.816203
276.169838	8000.433285	13.965517	-0.056326	4.816246
276.210530	8000.394492	13.970522	-0.056333	4.816234
276.287169	8000.415098	13.975527	-0.056348	4.816240
276.298236	8000.419564	13.980531	-0.056350	4.816241
276.188373	8000.364164	13.985536	-0.056329	4.816225
276.340663	8000.417113	13.990541	-0.056357	4.816240
276.317477	8000.283168	13.995546	-0.056353	4.816201
276.123882	8000.400363	14.000551	-0.056317	4.816236
276.406957	8000.370224	14.005555	-0.056369	4.816226
276.359920	8000.283915	14.010560	-0.056361	4.816201
276.119923	8000.447270	14.015565	-0.056316	4.816250
276.234359	8000.282701	14.020570	-0.056337	4.816201
276.510560	8000.427614	14.025575	-0.056388	4.816242
276.303993	8000.321331	14.030579	-0.056350	4.816212
276.194489	8000.297983	14.035584	-0.056329	4.816206
276.154099	8000.423287	14.040589	-0.056322	4.816243
276.183961	8000.215532	14.045594	-0.056327	4.816182
276.135810	8000.350309	14.050599	-0.056318	4.816222
276.360238	8000.219772	14.055603	-0.056360	4.816182
276.393547	8000.262025	14.060608	-0.056366	4.816194
276.165428	8000.377528	14.065613	-0.056324	4.816229
276.221861	8000.399905	14.070618	-0.056334	4.816236
276.267396	8000.362268	14.075623	-0.056342	4.816224
276.465725	8000.278257	14.080627	-0.056379	4.816199
276.348605	8000.245158	14.085632	-0.056357	4.816190
276.310139	8000.359816	14.090637	-0.056350	4.816223
276.402734	8000.215146	14.095642	-0.056367	4.816181
276.240751	8000.252802	14.100647	-0.056337	4.816192
276.163805	8000.148864	14.105651	-0.056323	4.816163
276.276607	8000.413659	14.110656	-0.056344	4.816239
276.312101	8000.363022	14.115661	-0.056350	4.816224
276.491823	8000.333151	14.120666	-0.056384	4.816215
276.439091	8000.392008	14.125671	-0.056374	4.816232
276.330544	8000.229817	14.130675	-0.056353	4.816185
276.361488	8000.296595	14.135680	-0.056359	4.816205
276.388595	8000.231921	14.140685	-0.056364	4.816186
276.619285	8000.168790	14.145690	-0.056407	4.816166
276.265276	8000.353584	14.150695	-0.056341	4.816222
276.297814	8000.391551	14.155699	-0.056347	4.816233
276.348405	8000.196988	14.160704	-0.056356	4.816176
276.339309	8000.355970	14.165709	-0.056355	4.816222
276.227192	8000.136037	14.170714	-0.056334	4.816158
276.348522	8000.224742	14.175719	-0.056356	4.816184
276.312470	8000.353329	14.180723	-0.056349	4.816222
276.332291	8000.349408	14.185728	-0.056353	4.816220
276.320643	8000.376963	14.190733	-0.056351	4.816228
276.447668	8000.253210	14.195738	-0.056374	4.816192
276.429931	8000.410970	14.200743	-0.056371	4.816238
276.323473	8000.191137	14.205747	-0.056351	4.816174
276.452299	8000.308818	14.210752	-0.056375	4.816208
276.427976	8000.499571	14.215757	-0.056371	4.816264
276.247264	8000.259169	14.220762	-0.056337	4.816194
276.380162	8000.426059	14.225767	-0.056361	4.816242
276.514036	8000.381473	14.230771	-0.056386	4.816229
276.491752	8000.393882	14.235776	-0.056382	4.816232
276.338589	8000.366539	14.240781	-0.056353	4.816225
276.431211	8000.326549	14.245786	-0.056371	4.816213
276.321044	8000.395049	14.250791	-0.056350	4.816234
276.358859	8000.422429	14.255795	-0.056357	4.816242
276.611072	7999.546840	14.260800	-0.056403	4.815984

276.444216	7996.245859	14.265805	-0.056370	4.815020
276.431981	7990.752281	14.270810	-0.056364	4.813414
276.437297	7983.971764	14.275815	-0.056361	4.811430
276.436038	7976.652085	14.280819	-0.056356	4.809288
276.273262	7969.071678	14.285824	-0.056320	4.807070
275.968105	7961.204687	14.290829	-0.056258	4.804767
276.196489	7953.401746	14.295834	-0.056296	4.802479
275.994957	7945.382337	14.300839	-0.056253	4.800129
275.977021	7937.438077	14.305843	-0.056244	4.797799
275.930871	7929.425974	14.310848	-0.056230	4.795448
276.023550	7921.375424	14.315853	-0.056242	4.793083
275.936933	7913.405645	14.320858	-0.056221	4.790743
275.793814	7905.418735	14.325863	-0.056189	4.788396
275.798610	7897.402019	14.330867	-0.056185	4.786038
275.754509	7889.425639	14.335872	-0.056171	4.783692
275.636837	7881.428755	14.340877	-0.056144	4.781338
275.916465	7873.438631	14.345882	-0.056191	4.778984
275.713049	7865.433555	14.350887	-0.056148	4.776626
275.774350	7857.440614	14.355891	-0.056154	4.774270
275.768512	7849.415716	14.360896	-0.056147	4.771903
275.471669	7841.344139	14.365901	-0.056087	4.769523
275.591630	7833.395672	14.370906	-0.056104	4.767175
275.602694	7825.354476	14.375911	-0.056101	4.764800
275.634736	7817.405242	14.380915	-0.056101	4.762451
275.422171	7809.409142	14.385920	-0.056056	4.760088
275.312917	7801.417414	14.390925	-0.056031	4.757724
275.296725	7793.394010	14.395930	-0.056022	4.755349
275.142455	7785.337020	14.400935	-0.055988	4.752964
275.219017	7777.310235	14.405939	-0.055997	4.750586
275.284469	7769.366286	14.410944	-0.056004	4.748231
275.321100	7761.311190	14.415949	-0.056006	4.745842
275.189849	7753.413810	14.420954	-0.055976	4.743499
275.052333	7745.367861	14.425959	-0.055945	4.741111
274.987162	7737.356295	14.430963	-0.055928	4.738732
274.965440	7729.386047	14.435968	-0.055919	4.736363
274.948952	7721.320128	14.440973	-0.055910	4.733965
274.995382	7713.369183	14.445978	-0.055914	4.731600
275.030032	7705.363346	14.450983	-0.055915	4.729218
274.764407	7697.317453	14.455987	-0.055860	4.726823
274.929688	7689.347317	14.460992	-0.055885	4.724448
274.734189	7681.348103	14.465997	-0.055844	4.722064
274.742142	7673.342505	14.471002	-0.055840	4.719677
274.575462	7665.358066	14.476007	-0.055804	4.717295
274.471895	7657.328157	14.481011	-0.055779	4.714898
274.570680	7649.329383	14.486016	-0.055792	4.712509
274.371425	7641.325596	14.491021	-0.055750	4.710118
274.507933	7633.349898	14.496026	-0.055770	4.707733
274.342909	7625.281600	14.501031	-0.055734	4.705320
274.125122	7617.332815	14.506035	-0.055688	4.702942
274.101753	7609.331428	14.511040	-0.055678	4.700546
274.332071	7601.335210	14.516045	-0.055716	4.698150
274.414415	7593.333457	14.521050	-0.055726	4.695751
274.221193	7585.289870	14.526055	-0.055685	4.693339
274.192088	7577.250731	14.531059	-0.055674	4.690927
274.047762	7569.324046	14.536064	-0.055642	4.688548
273.639891	7561.267538	14.541069	-0.055561	4.686129
273.796899	7553.310797	14.546074	-0.055585	4.683737
273.957860	7545.324877	14.551079	-0.055609	4.681336
273.746325	7537.311429	14.556083	-0.055565	4.678926
273.669752	7529.361161	14.561088	-0.055545	4.676533
273.702608	7521.254006	14.566093	-0.055546	4.674092
273.599336	7513.169926	14.571098	-0.055521	4.671656
273.412575	7505.181761	14.576103	-0.055481	4.669249
273.628879	7497.207373	14.581107	-0.055516	4.666843
273.638702	7489.251383	14.586112	-0.055513	4.664442
273.372308	7481.305239	14.591117	-0.055458	4.662044
273.291323	7473.238204	14.596122	-0.055438	4.659607
273.292002	7465.267749	14.601127	-0.055433	4.657198
273.329713	7457.240707	14.606131	-0.055434	4.654771
273.398394	7449.249969	14.611136	-0.055442	4.652353
273.266782	7441.178964	14.616141	-0.055412	4.649910
273.216131	7433.270276	14.621146	-0.055397	4.647515
273.189579	7425.227769	14.626151	-0.055387	4.645078
273.052877	7417.278643	14.631155	-0.055356	4.642668
272.927116	7409.227765	14.636160	-0.055328	4.640226
272.743165	7401.267368	14.641165	-0.055288	4.637810
272.858760	7393.263863	14.646170	-0.055304	4.635380
272.994491	7385.218352	14.651175	-0.055324	4.632935
272.824470	7377.155634	14.656179	-0.055287	4.630484
272.746360	7369.210389	14.661184	-0.055268	4.628068
272.760301	7361.185453	14.666189	-0.055265	4.625626
272.785341	7353.268323	14.671194	-0.055264	4.623215
272.542225	7345.213370	14.676199	-0.055214	4.620762
272.583813	7337.201223	14.681203	-0.055216	4.618320
272.615861	7329.205573	14.686208	-0.055217	4.615881
272.500395	7321.154592	14.691213	-0.055190	4.613425
272.525067	7313.177659	14.696218	-0.055189	4.610990
272.384338	7305.174100	14.701223	-0.055158	4.608545
272.265038	7297.170787	14.706227	-0.055130	4.606099
272.344833	7289.215813	14.711232	-0.055140	4.603667
272.044308	7281.170965	14.716237	-0.055079	4.601206
272.308229	7273.229635	14.721242	-0.055123	4.598775
271.853002	7265.192447	14.726247	-0.055032	4.596314
272.022117	7257.137294	14.731251	-0.055059	4.593846
272.229978	7249.112871	14.736256	-0.055092	4.591385
271.838007	7241.131623	14.741261	-0.055014	4.588937
271.749089	7233.145442	14.746266	-0.054992	4.586486
271.949678	7225.177555	14.751271	-0.055024	4.584039
272.166363	7217.169138	14.756275	-0.055059	4.581579
271.886656	7209.171657	14.761280	-0.055002	4.579120
271.836044	7201.139698	14.766285	-0.054987	4.576650
271.699812	7193.160927	14.771290	-0.054956	4.574194
271.702804	7185.113263	14.776295	-0.054952	4.571717
271.708442	7177.088200	14.781299	-0.054947	4.569244
271.782469	7169.127077	14.786304	-0.054956	4.566790
271.562212	7161.120323	14.791309	-0.054910	4.564321
271.456081	7153.216824	14.796314	-0.054885	4.561882
271.403115	7145.153681	14.801319	-0.054869	4.559392
271.516407	7137.179343	14.806323	-0.054885	4.556929
271.419498	7129.163502	14.811328	-0.054862	4.554452
271.376939	7121.113532	14.816333	-0.054849	4.551962
271.297228	7113.094352	14.821338	-0.054829	4.549481
271.096426	7105.098193	14.826343	-0.054786	4.547005
271.328877	7097.113819	14.831347	-0.054824	4.544532
271.217907	7089.230814	14.836352	-0.054798	4.542089
271.002171	7081.115023	14.841357	-0.054753	4.539572
271.301040	7073.196631	14.846362	-0.054803	4.537115
271.286839	7065.121033	14.851367	-0.054795	4.534608
271.096350	7057.142231	14.856371	-0.054754	4.532130
270.914683	7049.098535	14.861376	-0.054715	4.529630
270.845427	7041.131028	14.866381	-0.054697	4.527152
270.814511	7033.100493	14.871386	-0.054686	4.524654
270.714805	7025.165045	14.876391	-0.054662	4.522183
270.740184	7017.121007	14.881395	-0.054661	4.519678
270.684457	7009.173063	14.886400	-0.054646	4.517201
270.605329	7001.084516	14.891405	-0.054626	4.514679
270.540226	6993.038454	14.896410	-0.054608	4.512168
270.463144	6985.038978	14.901415	-0.054589	4.509671
270.427832	6977.096645	14.906419	-0.054577	4.507190
270.493846	6969.082083	14.911424	-0.054584	4.504686
270.371392	6961.104281	14.916429	-0.054556	4.502191
270.408824	6953.111802	14.921434	-0.054558	4.499690
270.316153	6945.112794	14.926439	-0.054535	4.497186
270.175343	6937.094752	14.931443	-0.054503	4.494675
270.300788	6929.054203	14.936448	-0.054522	4.492155
270.210819	6920.979098	14.941453	-0.054499	4.489623
270.063715	6913.075212	14.946458	-0.054467	4.487143
270.020660	6905.054554	14.951463	-0.054454	4.484625
269.915020	6897.100591	14.956467	-0.054429	4.482126
269.923847	6889.107370	14.961472	-0.054425	4.479614
269.983311	6881.070524	14.966477	-0.054431	4.477087
270.010074	6873.065294	14.971482	-0.054430	4.474569
269.774209	6865.034386	14.976487	-0.054381	4.472040
269.666050	6857.021728	14.981491	-0.054356	4.469516
269.605876	6849.041886	14.986496	-0.054339	4.467001
269.561228	6841.019892	14.991501	-0.054326	4.464471
269.596646	6833.063957	14.996506	-0.054327	4.461961
269.489595	6825.056664	15.001511	-0.054302	4.459433
269.409656	6817.057622	15.006515	-0.054282	4.456906
269.643917	6809.057721	15.011520	-0.054320	4.454378
269.569746	6801.012437	15.016525	-0.054301	4.451834
269.588187	6793.026960	15.021530	-0.054299	4.449307
269.481704	6785.021838	15.026535	-0.054274	4.446772
269.351561	6777.002889	15.031539	-0.054244	4.444232
269.356383	6769.023402	15.036544	-0.054240	4.441703
269.231993	6760.999849	15.041549	-0.054212	4.439158
269.421387	6753.056741	15.046554	-0.054242	4.436638
269.267553	6745.017211	15.051559	-0.054208	4.434085
269.038157	6736.964681	15.056563	-0.054160	4.431526
268.880024	6729.008275	15.061568	-0.054125	4.428996
268.764758	6720.967604	15.066573	-0.054098	4.426438
268.872651	6713.023784	15.071578	-0.054113	4.423910
268.975509	6704.999263	15.076583	-0.054127	4.421356
268.829280	6696.987670	15.081587	-0.054094	4.418802
268.793181	6689.000778	15.086592	-0.054082	4.416256
268.758140	6680.995994	15.091597	-0.054070	4.413703
268.860229	6672.981187	15.096602	-0.054084	4.411145
268.655526	6665.014547	15.101607	-0.054041	4.408600
268.551510	6656.963206	15.106611	-0.054016	4.406027
268.699969	6649.016327	15.111616	-0.054039	4.403487
268.348205	6640.984958	15.116621	-0.053968	4.400916
268.231071	6633.028942	15.121626	-0.053941	4.398369
268.392337	6624.993364	15.126631	-0.053965	4.395796
268.477859	6616.966545	15.131635	-0.053976	4.393224
268.509236	6608.967650	15.136640	-0.053977	4.390659
268.330033	6600.975840	15.141645	-0.053938	4.388094
268.223119	6592.981772	15.146650	-0.053913	4.385527
268.004581	6585.007879	15.151655	-0.053867	4.382965
268.224638	6576.964426	15.156659	-0.053902	4.380381
268.286723	6569.046704	15.161664	-0.053909	4.377835
268.052317	6560.965988	15.166669	-0.053860	4.375233
268.235883	6552.996376	15.171674	-0.053889	4.372668
268.081707	6544.964615	15.176679	-0.053855	4.370080
267.761171	6537.000649	15.181683	-0.053790	4.367510
267.739614	6529.020685	15.186688	-0.053781	4.364936
267.834908	6521.023996	15.191693	-0.053793	4.362356
267.905084	6513.010238	15.196698	-0.053801	4.359768
267.611858	6505.058144	15.201703	-0.053741	4.357197
267.753152	6496.980178	15.206707	-0.053762	4.354586
267.611218	6488.923918	15.211712	-0.053730	4.351979
267.369342	6480.896630	15.216717	-0.053680	4.349379
267.608533	6472.940158	15.221722	-0.053719	4.346803
267.377492	6464.923294	15.226727	-0.053671	4.344204
267.224411	6456.923274	15.231731	-0.053637	4.341608
267.399388	6448.982207	15.236736	-0.053664	4.339033
267.312341	6440.985666	15.241741	-0.053643	4.336436
267.324520	6432.947763	15.246746	-0.053640	4.333825
267.188376	6424.959018	15.251751	-0.053609	4.331227
267.216560	6416.966948	15.256755	-0.053609	4.328627
267.213949	6408.963054	15.261760	-0.053603	4.326022
266.871761	6400.950030	15.266765	-0.053534	4.323411
266.880800	6392.986278	15.271770	-0.053531	4.320816
266.683970	6385.007784	15.276775	-0.053489	4.318213
266.703108	6376.965436	15.281779	-0.053487	4.315589
266.459274	6368.958560	15.286784	-0.053436	4.312973
266.441305	6360.903915	15.291789	-0.053428	4.310342
266.618979	6352.955861	15.296794	-0.053456	4.307746
266.459711	6344.912230	15.301799	-0.053421	4.305114
266.328117	6336.940680	15.306803	-0.053391	4.302504
266.441018	6328.936062	15.311808	-0.053407	4.299884
266.364426	6320.938727	15.316813	-0.053387	4.297263
266.435892	6312.953357	15.321818	-0.053395	4.294645
266.525798	6304.931494	15.326823	-0.053407	4.292014
266.318125	6296.914866	15.331827	-0.053363	4.289381
266.091293	6288.960719	15.336832	-0.053315	4.286767
266.176299	6280.909106	15.341837	-0.053326	4.284121
266.347506	6272.952419	15.346842	-0.053352	4.281506
266.355215	6264.934319	15.351847	-0.053348	4.278868
266.203760	6256.956348	15.356851	-0.053315	4.276240
266.187013	6248.911821	15.361856	-0.053306	4.273589
266.121628	6240.848896	15.366861	-0.053289	4.270930
266.031230	6232.896672	15.371866	-0.053267	4.268306
266.059534	6224.884923	15.376871	-0.053267	4.265662
265.982065	6216.913905	15.381875	-0.053247	4.263029
265.801594	6208.932554	15.386880	-0.053208	4.260389
265.696795	6200.970316	15.391885	-0.053184	4.257755
265.877481	6192.895267	15.396890	-0.053212	4.255085
265.697288	6184.901619	15.401895	-0.053173	4.252436
265.576279	6176.870019	15.406899	-0.053145	4.249774
265.683282	6168.978644	15.411904	-0.053160	4.247159
265.703393	6160.890269	15.416909	-0.053158	4.244476
265.669856	6152.964534	15.421914	-0.053147	4.241844
265.615357	6144.920279	15.426919	-0.053131	4.239172
265.499136	6136.995503	15.431923	-0.053104	4.236537
265.507077	6128.925886	15.436928	-0.053101	4.233853
265.427021	6120.885408	15.441933	-0.053080	4.231177
265.489575	6112.923856	15.446938	-0.053087	4.228526
265.293296	6104.938049	15.451943	-0.053045	4.225864
265.164298	6096.943284	15.456947	-0.053016	4.223197
265.188837	6088.959529	15.461952	-0.053015	4.220533
265.134589	6080.941011	15.466957	-0.053000	4.217856
265.165066	6072.944778	15.471962	-0.053000	4.215185
264.810583	6064.956439	15.476967	-0.052929	4.212511
264.922064	6056.900851	15.481971	-0.052944	4.209818
264.967531	6048.985681	15.486976	-0.052947	4.207169
264.820587	6040.893898	15.491981	-0.052915	4.204458
264.877600	6033.018287	15.496986	-0.052920	4.201819
264.861089	6024.981364	15.501991	-0.052912	4.199124
264.569881	6016.969116	15.506995	-0.052852	4.196432
264.471084	6008.908852	15.512000	-0.052828	4.193725
264.493283	6000.785099	15.517005	-0.052827	4.190996
264.708891	5992.889944	15.522010	-0.052862	4.188344
264.483321	5984.866865	15.527015	-0.052815	4.185642
264.124985	5976.954282	15.532019	-0.052743	4.182975
264.369444	5968.914862	15.537024	-0.052783	4.180269
264.096841	5960.931215	15.542029	-0.052727	4.177575
264.184911	5952.902463	15.547034	-0.052738	4.174868
264.017627	5944.933326	15.552039	-0.052702	4.172177
263.902399	5936.866999	15.557043	-0.052675	4.169451
263.849678	5928.943418	15.562048	-0.052660	4.166773
263.903299	5920.869204	15.567053	-0.052665	4.164043
263.839684	5912.936939	15.572058	-0.052648	4.161358
263.912301	5904.944487	15.577063	-0.052656	4.158652
263.770949	5896.901701	15.582067	-0.052624	4.155926
263.832639	5888.850098	15.587072	-0.052630	4.153196
263.623495	5880.902119	15.592077	-0.052586	4.150497
263.877520	5872.876609	15.597082	-0.052628	4.147776
263.988600	5864.830823	15.602087	-0.052644	4.145044
263.903140	5856.897107	15.607091	-0.052622	4.142346
263.659638	5848.930009	15.612096	-0.052572	4.139633
263.464947	5840.924375	15.617101	-0.052530	4.136905
263.367365	5832.898735	15.622106	-0.052507	4.134170
263.298385	5824.904921	15.627111	-0.052489	4.131445
263.426401	5816.885686	15.632115	-0.052507	4.128711
263.602545	5808.888301	15.637120	-0.052535	4.125984
263.358691	5800.901963	15.642125	-0.052484	4.123253
263.369514	5792.914640	15.647130	-0.052481	4.120524
263.259798	5784.972547	15.652135	-0.052455	4.117806
263.291095	5776.899314	15.657139	-0.052456	4.115044
263.236778	5768.900234	15.662144	-0.052440	4.112304
263.257165	5760.852777	15.667149	-0.052439	4.109547
262.958277	5752.908936	15.672154	-0.052378	4.106819
262.956203	5744.901311	15.677159	-0.052372	4.104071
263.045708	5736.882018	15.682163	-0.052383	4.101319
262.899276	5728.943208	15.687168	-0.052351	4.098590
262.655683	5720.919909	15.692173	-0.052300	4.095828
262.958292	5712.905991	15.697178	-0.052351	4.093074
262.847481	5704.872252	15.702183	-0.052325	4.090307
262.789792	5696.923506	15.707187	-0.052309	4.087568
262.631580	5688.892543	15.712192	-0.052275	4.084797
262.696590	5680.955295	15.717197	-0.052282	4.082060
262.615049	5672.942241	15.722202	-0.052261	4.079292
262.408350	5665.021753	15.727207	-0.052217	4.076553
262.528291	5656.914236	15.732211	-0.052234	4.073752
262.674447	5648.906854	15.737216	-0.052256	4.070984
262.340780	5640.922030	15.742221	-0.052189	4.068216
262.498781	5632.906137	15.747226	-0.052213	4.065441
262.506376	5624.972791	15.752231	-0.052209	4.062691
262.114229	5616.951987	15.757235	-0.052131	4.059904
262.146145	5609.008783	15.762240	-0.052132	4.057147
261.975075	5600.968677	15.767245	-0.052094	4.054352
262.091042	5592.918921	15.772250	-0.052111	4.051556
262.147576	5584.903133	15.777255	-0.052116	4.048768
262.197487	5576.885947	15.782259	-0.052120	4.045978
262.218673	5568.947146	15.787264	-0.052119	4.043214
261.865838	5560.914677	15.792269	-0.052048	4.040409
262.056056	5552.968208	15.797274	-0.052078	4.037640
261.942297	5544.961159	15.802279	-0.052051	4.034844
261.555327	5536.830926	15.807283	-0.051974	4.031998
261.606525	5528.895236	15.812288	-0.051978	4.029225
261.695635	5520.891111	15.817293	-0.051989	4.026427
261.766377	5512.925403	15.822298	-0.051997	4.023640
261.804991	5504.917562	15.827303	-0.051999	4.020836
261.634620	5496.939430	15.832307	-0.051962	4.018037
261.702610	5488.921928	15.837312	-0.051970	4.015226
261.358619	5480.922579	15.842317	-0.051900	4.012413
261.273143	5472.881282	15.847322	-0.051879	4.009587
261.464148	5464.941907	15.852327	-0.051909	4.006800
261.352488	5456.889099	15.857331	-0.051883	4.003965
261.005102	5448.961532	15.862336	-0.051813	4.001170
261.038267	5440.960734	15.867341	-0.051814	3.998352
261.012672	5432.959337	15.872346	-0.051804	3.995531
261.004455	5424.895586	15.877351	-0.051797	3.992687
261.009040	5416.849394	15.882355	-0.051793	3.989847
261.132712	5408.933434	15.887360	-0.051811	3.987053
261.038624	5400.889831	15.892365	-0.051788	3.984208
260.901768	5392.947490	15.897370	-0.051757	3.981396
260.760147	5384.944038	15.902375	-0.051726	3.978561
260.675263	5376.950799	15.907379	-0.051704	3.975728
260.633330	5368.931384	15.912384	-0.051691	3.972884
260.821937	5360.891211	15.917389	-0.051721	3.970035
260.866010	5352.962808	15.922394	-0.051724	3.967221
260.840391	5344.945763	15.927399	-0.051714	3.964373
260.621534	5337.003266	15.932403	-0.051668	3.961545
260.639738	5329.010624	15.937408	-0.051666	3.958702
260.387100	5320.981319	15.942413	-0.051614	3.955839
260.299888	5312.957086	15.947418	-0.051592	3.952979
260.287116	5304.959661	15.952423	-0.051585	3.950127
260.174605	5296.955311	15.957427	-0.051558	3.947269
260.085210	5288.993284	15.962432	-0.051536	3.944425
260.011789	5280.973388	15.967437	-0.051518	3.941558
260.187970	5272.980423	15.972442	-0.051545	3.938703
259.998330	5264.998793	15.977447	-0.051504	3.935844
259.821610	5256.956186	15.982451	-0.051466	3.932960
260.129015	5248.956751	15.987456	-0.051518	3.930099
260.150659	5240.969271	15.992461	-0.051517	3.927235
259.891189	5233.005875	15.997466	-0.051463	3.924372
259.749962	5225.032105	16.002471	-0.051432	3.921506
259.877183	5217.015243	16.007475	-0.051450	3.918627
259.912593	5209.047000	16.012480	-0.051452	3.915762
259.669882	5201.010990	16.017485	-0.051401	3.912865
259.740151	5192.963517	16.022490	-0.051409	3.909967
259.512557	5185.024516	16.027495	-0.051361	3.907101
259.418150	5176.982589	16.032499	-0.051338	3.904198
259.636953	5169.035303	16.037504	-0.051374	3.901333
259.404878	5160.999390	16.042509	-0.051325	3.898426
259.146002	5153.023612	16.047514	-0.051272	3.895537
259.400844	5144.989392	16.052519	-0.051314	3.892635
259.346371	5136.945203	16.057523	-0.051299	3.889721
259.286056	5129.027950	16.062528	-0.051282	3.886851
259.233924	5120.981035	16.067533	-0.051267	3.883932
259.220286	5113.013857	16.072538	-0.051259	3.881041
259.305036	5105.043158	16.077543	-0.051270	3.878147
259.002162	5096.988077	16.082547	-0.051208	3.875214
258.999401	5088.810071	16.087552	-0.051202	3.872239
258.931247	5080.834739	16.092557	-0.051184	3.869335
258.976043	5072.916801	16.097562	-0.051187	3.866451
258.719232	5064.942160	16.102567	-0.051134	3.863539
258.822012	5056.939769	16.107571	-0.051148	3.860622
258.876440	5049.009252	16.112576	-0.051153	3.857727
258.651643	5040.975094	16.117581	-0.051106	3.854787
258.838190	5032.984550	16.122586	-0.051135	3.851869
258.788580	5025.017989	16.127591	-0.051121	3.848953
258.553756	5016.989235	16.132595	-0.051072	3.846008
258.740819	5009.045740	16.137600	-0.051101	3.843100
258.490363	5001.037011	16.142605	-0.051049	3.840158
258.371069	4993.046832	16.147610	-0.051022	3.837223
258.472540	4985.066707	16.152615	-0.051036	3.834293
258.208583	4977.023024	16.157619	-0.050981	3.831331
258.320635	4969.051177	16.162624	-0.050997	3.828400
258.221658	4961.020105	16.167629	-0.050973	3.825441
258.122078	4953.056310	16.172634	-0.050949	3.822505
258.122956	4945.065926	16.177639	-0.050944	3.819558
257.943191	4937.114790	16.182643	-0.050905	3.816620
258.005211	4929.103716	16.187648	-0.050912	3.813662
258.093914	4921.036521	16.192653	-0.050923	3.810682
258.024468	4913.093497	16.197658	-0.050905	3.807743
257.978668	4905.086158	16.202663	-0.050891	3.804778
257.756285	4897.125599	16.207667	-0.050844	3.801823
257.825671	4889.113201	16.212672	-0.050852	3.798854
257.642472	4881.140214	16.217677	-0.050812	3.795892
257.367084	4873.099076	16.222682	-0.050756	3.792900
257.632065	4865.042055	16.227687	-0.050800	3.789911
257.439371	4857.034908	16.232691	-0.050759	3.786928
257.443865	4849.082079	16.237696	-0.050754	3.783968
257.414699	4841.067935	16.242701	-0.050743	3.780982
257.478358	4833.104867	16.247706	-0.050750	3.778014
257.576030	4825.087464	16.252711	-0.050763	3.775025
257.611931	4817.105967	16.257715	-0.050764	3.772045
257.480668	4809.107366	16.262720	-0.050735	3.769053
257.232409	4801.084656	16.267725	-0.050683	3.766047
256.928877	4793.157669	16.272730	-0.050621	3.763073
256.765307	4785.122834	16.277735	-0.050586	3.760060
256.661410	4777.157493	16.282739	-0.050561	3.757071
256.757394	4769.098227	16.287744	-0.050574	3.754049
256.783225	4761.089583	16.292749	-0.050573	3.751042
256.777578	4753.107552	16.297754	-0.050567	3.748042
256.777527	4745.083453	16.302759	-0.050561	3.745024
256.828018	4737.109972	16.307763	-0.050566	3.742024
256.696903	4729.166516	16.312768	-0.050536	3.739028
256.493516	4721.145402	16.317773	-0.050493	3.735999
256.647437	4713.164916	16.322778	-0.050516	3.732992
256.650216	4705.118414	16.327783	-0.050511	3.729953
256.610766	4697.145522	16.332787	-0.050499	3.726939
256.555276	4689.204861	16.337792	-0.050483	3.723934
256.553100	4681.166712	16.342797	-0.050477	3.720891
256.468386	4673.214490	16.347802	-0.050456	3.717876
256.187660	4665.216159	16.352807	-0.050399	3.714836
255.935929	4657.100137	16.357811	-0.050347	3.711750
256.002220	4649.111215	16.362816	-0.050354	3.708718
255.952831	4641.111572	16.367821	-0.050339	3.705675
255.986928	4633.173874	16.372826	-0.050340	3.702656
256.116694	4625.156166	16.377831	-0.050359	3.699607
255.928671	4617.199094	16.382835	-0.050319	3.696570
255.846311	4609.210720	16.387840	-0.050298	3.693522
255.895623	4601.147673	16.392845	-0.050302	3.690445
255.802716	4593.215776	16.397850	-0.050280	3.687413
255.750438	4585.188218	16.402855	-0.050265	3.684342
255.734737	4577.241648	16.407859	-0.050256	3.681301
255.870020	4569.249368	16.412864	-0.050276	3.678244
255.437480	4561.257117	16.417869	-0.050191	3.675169
255.517345	4553.229764	16.422874	-0.050200	3.672092
255.473802	4545.214036	16.427879	-0.050187	3.669013
255.658113	4537.203726	16.432883	-0.050216	3.665940
255.555125	4529.263026	16.437888	-0.050191	3.662884
255.381660	4521.225883	16.442893	-0.050154	3.659786
255.334286	4513.294108	16.447898	-0.050140	3.656729
255.084504	4505.272522	16.452903	-0.050088	3.653630
255.118690	4497.204745	16.457907	-0.050089	3.650517
255.358595	4489.268908	16.462912	-0.050128	3.647459
255.136277	4481.252296	16.467917	-0.050082	3.644354
254.837363	4473.308331	16.472922	-0.050021	3.641273
254.961534	4465.302069	16.477927	-0.050039	3.638177
254.918786	4457.268898	16.482931	-0.050025	3.635062
254.912091	4449.264301	16.487936	-0.050019	3.631957
254.812418	4441.252053	16.492941	-0.049995	3.628845
254.668625	4433.248169	16.497946	-0.049963	3.625731
254.584095	4425.303307	16.502951	-0.049942	3.622639
254.492411	4417.276765	16.507955	-0.049920	3.619513
254.574238	4409.332455	16.512960	-0.049930	3.616421
254.345944	4401.309290	16.517965	-0.049882	3.613286
254.287873	4393.312474	16.522970	-0.049866	3.610164
254.357046	4385.338450	16.527975	-0.049873	3.607052
254.250994	4377.314953	16.532979	-0.049848	3.603913
254.329336	4369.363662	16.537984	-0.049858	3.600804
254.192889	4361.386586	16.542989	-0.049827	3.597677
254.250489	4353.395580	16.547994	-0.049832	3.594547
254.079769	4345.375250	16.552999	-0.049795	3.591396
254.117077	4337.351175	16.558003	-0.049797	3.588247
254.115313	4329.382197	16.563008	-0.049791	3.585116
253.971268	4321.397861	16.568013	-0.049759	3.581971
253.949370	4313.403100	16.573018	-0.049750	3.578824
254.002050	4305.410803	16.578023	-0.049754	3.575677
253.708939	4297.388010	16.583027	-0.049694	3.572505
253.591124	4289.409584	16.588032	-0.049667	3.569352
253.656719	4281.409921	16.593037	-0.049674	3.566194
253.616587	4273.437657	16.598042	-0.049661	3.563041
253.572845	4265.411229	16.603047	-0.049648	3.559863
253.501865	4257.449929	16.608051	-0.049630	3.556708
253.626857	4249.381361	16.613056	-0.049648	3.553513
253.532956	4241.307028	16.618061	-0.049625	3.550306
253.297084	4233.390388	16.623066	-0.049576	3.547155
253.314866	4225.413436	16.628071	-0.049574	3.543985
253.286546	4217.404689	16.633075	-0.049563	3.540797
253.214751	4209.466748	16.638080	-0.049544	3.537634
252.980017	4201.449460	16.643085	-0.049495	3.534432
253.244565	4193.411569	16.648090	-0.049539	3.531233
253.105105	4185.449457	16.653095	-0.049508	3.528049
252.956563	4177.447656	16.658099	-0.049475	3.524847
253.070808	4169.477844	16.663104	-0.049491	3.521662
253.130527	4161.465540	16.668109	-0.049497	3.518456
252.881737	4153.497148	16.673114	-0.049445	3.515255
252.870652	4145.489279	16.678119	-0.049438	3.512042
252.797264	4137.460076	16.683123	-0.049419	3.508816
252.940306	4129.481551	16.688128	-0.049441	3.505614
252.785531	4121.523759	16.693133	-0.049406	3.502409
252.884926	4113.522807	16.698138	-0.049420	3.499191
252.792827	4105.562503	16.703143	-0.049397	3.495980
252.537242	4097.559511	16.708147	-0.049344	3.492744
252.503083	4089.564703	16.713152	-0.049333	3.489515
252.546218	4081.589854	16.718157	-0.049336	3.486294
252.162281	4073.618542	16.723162	-0.049259	3.483058
252.437053	4065.556446	16.728167	-0.049305	3.479802
252.395252	4057.604294	16.733171	-0.049292	3.476579
252.389591	4049.603625	16.738176	-0.049285	3.473333
252.196060	4041.536039	16.743181	-0.049244	3.470052
252.220728	4033.560359	16.748186	-0.049243	3.466811
252.158276	4025.595172	16.753191	-0.049226	3.463569
252.075746	4017.595377	16.758195	-0.049206	3.460310
252.203978	4009.641578	16.763200	-0.049224	3.457073
251.967945	4001.606330	16.768205	-0.049175	3.453787
252.009074	3993.605661	16.773210	-0.049177	3.450522
251.833131	3985.640589	16.778215	-0.049139	3.447261
251.717110	3977.613500	16.783219	-0.049112	3.443974
251.623911	3969.675371	16.788224	-0.049090	3.440720
251.600676	3961.658461	16.793229	-0.049080	3.437434
251.494314	3953.671155	16.798234	-0.049055	3.434153
251.540441	3945.672361	16.803239	-0.049058	3.430870
251.158291	3937.669625	16.808243	-0.048982	3.427568
251.261001	3929.694533	16.813248	-0.048996	3.424290
251.264143	3921.663922	16.818253	-0.048991	3.420983
251.406581	3913.700860	16.823258	-0.049012	3.417705
251.210776	3905.729203	16.828263	-0.048971	3.414409
251.161114	3897.687618	16.833267	-0.048956	3.411086
251.072197	3889.723546	16.838272	-0.048934	3.407791
250.864050	3881.715225	16.843277	-0.048890	3.404470
250.953641	3873.783625	16.848282	-0.048902	3.401187
250.879002	3865.789712	16.853287	-0.048883	3.397870
250.880418	3857.750716	16.858291	-0.048878	3.394534
250.786395	3849.703537	16.863296	-0.048855	3.391187
250.783217	3841.712298	16.868301	-0.048849	3.387864
250.778731	3833.742510	16.873306	-0.048843	3.384546
250.643010	3825.812511	16.878311	-0.048812	3.381237
250.601517	3817.817339	16.883315	-0.048799	3.377901
250.618483	3809.834137	16.888320	-0.048797	3.374568
250.583082	3801.797530	16.893325	-0.048785	3.371208
250.496894	3793.817262	16.898330	-0.048764	3.367867
250.262019	3785.847880	16.903335	-0.048715	3.364521
250.064487	3777.898255	16.908339	-0.048673	3.361182
250.252653	3769.871718	16.913344	-0.048703	3.357821
250.213248	3761.848787	16.918349	-0.048690	3.354450
250.270238	3753.830149	16.923354	-0.048695	3.351081
250.199977	3745.857900	16.928359	-0.048677	3.347723
250.267180	3737.832986	16.933363	-0.048684	3.344345
250.157060	3729.923924	16.938368	-0.048658	3.341005
249.844551	3721.949379	16.943373	-0.048595	3.337628
249.908214	3713.925398	16.948378	-0.048602	3.334239
250.026381	3705.905558	16.953383	-0.048618	3.330851
249.928883	3697.900782	16.958387	-0.048595	3.327458
249.967923	3689.935763	16.963392	-0.048597	3.324084
249.845331	3681.959836	16.968397	-0.048569	3.320695
249.952243	3673.997008	16.973402	-0.048583	3.317317
249.891984	3666.004063	16.978407	-0.048567	3.313917
249.826549	3657.947957	16.983411	-0.048549	3.310485
249.772477	3649.976144	16.988416	-0.048534	3.307087
249.637166	3641.988998	16.993421	-0.048504	3.303676
249.445273	3634.029796	16.998426	-0.048463	3.300271
249.518049	3626.051783	17.003431	-0.048471	3.296864
249.261997	3618.047753	17.008435	-0.048418	3.293430
249.126395	3610.061144	17.013440	-0.048387	3.290005
249.242010	3602.067046	17.018445	-0.048404	3.286582
249.190750	3594.085248	17.023450	-0.048389	3.283155
249.077533	3586.102841	17.028455	-0.048362	3.279721
249.010398	3578.128340	17.033459	-0.048345	3.276289
249.089340	3570.117909	17.038464	-0.048354	3.272843
248.923767	3562.086539	17.043469	-0.048318	3.269376
248.762186	3554.104640	17.048474	-0.048283	3.265926
248.926586	3546.139283	17.053479	-0.048308	3.262492
248.820524	3538.141121	17.058483	-0.048283	3.259030
248.818537	3530.168718	17.063488	-0.048277	3.255580
248.779998	3522.145446	17.068493	-0.048265	3.252102
248.806713	3514.153592	17.073498	-0.048265	3.248637
248.727932	3506.175609	17.078503	-0.048245	3.245170
248.595755	3498.221146	17.083507	-0.048215	3.241708
248.800409	3490.222031	17.088512	-0.048248	3.238235
248.536770	3482.237322	17.093517	-0.048193	3.234747
248.454032	3474.184537	17.098522	-0.048172	3.231232
248.501640	3466.204261	17.103527	-0.048176	3.227751
248.388392	3458.193232	17.108531	-0.048150	3.224245
248.170763	3450.274146	17.113536	-0.048104	3.220772
248.011940	3442.290546	17.118541	-0.048069	3.217269
247.872007	3434.313960	17.123546	-0.048038	3.213766
247.792214	3426.310658	17.128551	-0.048018	3.210250
247.645461	3418.313923	17.133555	-0.047985	3.206730
247.947236	3410.298802	17.138560	-0.048036	3.203217
247.760709	3402.333339	17.143565	-0.047996	3.199702
247.580492	3394.391702	17.148570	-0.047957	3.196193
247.883139	3386.322026	17.153575	-0.048008	3.192645
247.894797	3378.305691	17.158579	-0.048005	3.189103
247.778488	3370.353436	17.163584	-0.047978	3.185581
247.551137	3362.405097	17.168589	-0.047931	3.182052
247.501522	3354.410038	17.173594	-0.047916	3.178506
247.519295	3346.413275	17.178599	-0.047914	3.174957
247.270779	3338.434075	17.183603	-0.047863	3.171402
247.611546	3330.408844	17.188608	-0.047921	3.167847
247.493225	3322.425358	17.193613	-0.047893	3.164287
247.120796	3314.497084	17.198618	-0.047819	3.160736
247.207861	3306.516096	17.203623	-0.047830	3.157178
247.177667	3298.473693	17.208627	-0.047819	3.153584
247.061123	3290.461400	17.213632	-0.047792	3.149995
247.001432	3282.493193	17.218637	-0.047775	3.146424
247.006844	3274.495024	17.223642	-0.047771	3.142838
247.163881	3266.530135	17.228647	-0.047795	3.139270
246.953338	3258.517769	17.233651	-0.047751	3.135660
247.017146	3250.549622	17.238656	-0.047757	3.132078
246.831099	3242.552014	17.243661	-0.047717	3.128468
246.733607	3234.590326	17.248666	-0.047694	3.124874
246.774495	3226.643583	17.253671	-0.047696	3.121288
246.581914	3218.664083	17.258675	-0.047655	3.117673
246.647811	3210.638056	17.263680	-0.047662	3.114044
246.511411	3202.640005	17.268685	-0.047631	3.110415
246.318384	3194.675554	17.273690	-0.047590	3.106794
246.349114	3186.689314	17.278695	-0.047591	3.103169
246.236449	3178.691671	17.283699	-0.047564	3.099528
246.268031	3170.724053	17.288704	-0.047565	3.095903
246.239915	3162.686816	17.293709	-0.047555	3.092240
246.129423	3154.719351	17.298714	-0.047529	3.088600
246.118056	3146.732261	17.303719	-0.047521	3.084951
246.107068	3138.771648	17.308723	-0.047514	3.081310
246.024936	3130.815353	17.313728	-0.047493	3.077664
246.170479	3122.765908	17.318733	-0.047515	3.073981
245.936297	3114.710739	17.323738	-0.047466	3.070273
246.050317	3106.745570	17.328743	-0.047482	3.066618
245.724437	3098.796529	17.333747	-0.047416	3.062946
245.828247	3090.836505	17.338752	-0.047430	3.059285
245.918755	3082.837248	17.343757	-0.047442	3.055600
245.833979	3074.843196	17.348762	-0.047421	3.051905
245.555624	3066.900952	17.353767	-0.047364	3.048221
245.507681	3058.884837	17.358771	-0.047350	3.044508
245.776884	3050.924057	17.363776	-0.047395	3.040832
245.397624	3042.971575	17.368781	-0.047319	3.037124
245.430969	3034.964296	17.373786	-0.047320	3.033406
245.558444	3026.942339	17.378791	-0.047338	3.029682
245.353495	3018.955875	17.383795	-0.047295	3.025953
245.215172	3011.013277	17.388800	-0.047264	3.022243
245.278076	3003.011478	17.393805	-0.047270	3.018510
245.278146	2995.012735	17.398810	-0.047265	3.014772
245.332024	2987.022306	17.403815	-0.047270	3.011035
245.147176	2979.041405	17.408819	-0.047230	3.007287
245.129981	2971.087589	17.413824	-0.047221	3.003554
244.804213	2963.128864	17.418829	-0.047155	2.999800
244.922728	2955.136923	17.423834	-0.047172	2.996047
244.850029	2947.135305	17.428839	-0.047153	2.992275
244.632036	2939.118110	17.433843	-0.047108	2.988484
244.546418	2931.154716	17.438848	-0.047086	2.984720
244.673366	2923.163738	17.443853	-0.047105	2.980949
244.692524	2915.190280	17.448858	-0.047103	2.977176
244.532658	2907.227502	17.453863	-0.047068	2.973394
244.426213	2899.219284	17.458867	-0.047043	2.969589
244.596639	2891.231274	17.463872	-0.047069	2.965802
244.316204	2883.277263	17.468877	-0.047012	2.962004
244.341016	2875.297669	17.473882	-0.047011	2.958204
244.411601	2867.309673	17.478887	-0.047019	2.954398
244.009195	2859.308251	17.483891	-0.046939	2.950556
244.130389	2851.321814	17.488896	-0.046956	2.946743
244.120405	2843.343499	17.493901	-0.046949	2.942922
244.112581	2835.377271	17.498906	-0.046942	2.939103
244.021347	2827.423927	17.503911	-0.046920	2.935280
243.818523	2819.406762	17.508915	-0.046877	2.931415
243.853774	2811.431475	17.513920	-0.046878	2.927578
243.671022	2803.457966	17.518925	-0.046839	2.923726
243.655257	2795.469763	17.523930	-0.046831	2.919870
243.829881	2787.524930	17.528935	-0.046858	2.916040
243.723488	2779.441920	17.533939	-0.046833	2.912123
243.417660	2771.474749	17.538944	-0.046771	2.908246
243.586131	2763.468898	17.543949	-0.046797	2.904371
243.610181	2755.512635	17.548954	-0.046796	2.900507
243.438005	2747.578949	17.553959	-0.046759	2.896638
243.363595	2739.572159	17.558963	-0.046740	2.892734
243.426861	2731.594265	17.563968	-0.046746	2.888846
243.231814	2723.615432	17.568973	-0.046705	2.884938
243.183326	2715.665070	17.573978	-0.046690	2.881046
243.214002	2707.694389	17.578983	-0.046691	2.877144
243.140195	2699.657708	17.583987	-0.046672	2.873199
243.083390	2691.673409	17.588992	-0.046656	2.869274
242.905621	2683.705960	17.593997	-0.046617	2.865346
242.846423	2675.761610	17.599002	-0.046601	2.861431
242.730643	2667.800345	17.604007	-0.046574	2.857498
242.720180	2659.787107	17.609011	-0.046567	2.853540
242.757599	2651.806106	17.614016	-0.046569	2.849596
242.741232	2643.817623	17.619021	-0.046560	2.845639
242.651283	2635.871841	17.624026	-0.046538	2.841694
242.677360	2627.912721	17.629031	-0.046538	2.837743
242.475087	2619.902690	17.634035	-0.046495	2.833748
242.412516	2611.918919	17.639040	-0.046478	2.829769
242.368556	2603.924905	17.644045	-0.046465	2.825780
242.412998	2595.950884	17.649050	-0.046468	2.821800
242.257445	2588.005895	17.654055	-0.046434	2.817818
242.418758	2579.979350	17.659059	-0.046458	2.813808
242.276774	2571.997608	17.664064	-0.046427	2.809796
242.018554	2564.058675	17.669069	-0.046373	2.805794
241.872579	2556.086693	17.674074	-0.046341	2.801776
241.808999	2548.144627	17.679079	-0.046324	2.797772
241.659987	2540.142162	17.684083	-0.046291	2.793727
241.925561	2532.110336	17.689088	-0.046335	2.789685
241.940132	2524.122707	17.694093	-0.046332	2.785646
241.890421	2516.162719	17.699098	-0.046318	2.781610
241.824104	2508.216234	17.704103	-0.046300	2.777575
241.580833	2500.235571	17.709107	-0.046250	2.773505
241.685623	2492.242819	17.714112	-0.046264	2.769445
241.543014	2484.274642	17.719117	-0.046232	2.765376
241.454089	2476.320563	17.724122	-0.046210	2.761311
241.654626	2468.337688	17.729127	-0.046242	2.757243
241.461620	2460.329675	17.734131	-0.046201	2.753133
241.413198	2452.315552	17.739136	-0.046187	2.749022
241.292371	2444.351727	17.744141	-0.046159	2.744926
241.225103	2436.400226	17.749146	-0.046141	2.740834
241.328068	2428.427240	17.754151	-0.046155	2.736734
241.117742	2420.442640	17.759155	-0.046111	2.732604
241.224285	2412.458121	17.764160	-0.046125	2.728487
240.788618	2404.520878	17.769165	-0.046039	2.724354
240.751482	2396.575731	17.774170	-0.046027	2.720236
240.993879	2388.586563	17.779175	-0.046067	2.716106
240.838094	2380.580564	17.784179	-0.046032	2.711936
240.957927	2372.586469	17.789184	-0.046049	2.707783
240.898465	2364.627778	17.794189	-0.046033	2.703631
240.884657	2356.656760	17.799194	-0.046025	2.699470
240.794155	2348.734082	17.804199	-0.046003	2.695322
240.459117	2340.751721	17.809203	-0.045935	2.691121
240.713552	2332.743866	17.814208	-0.045978	2.686937
240.474893	2324.792861	17.819213	-0.045928	2.682745
240.214925	2316.859360	17.824218	-0.045874	2.678555
240.324785	2308.870065	17.829223	-0.045889	2.674352
240.498809	2300.797428	17.834227	-0.045916	2.670103
240.300694	2292.879421	17.839232	-0.045874	2.665905
240.240836	2284.906544	17.844237	-0.045858	2.661680
240.187794	2276.954943	17.849242	-0.045843	2.657460
239.979998	2268.988445	17.854247	-0.045799	2.653215
239.797240	2261.001854	17.859251	-0.045760	2.648954
239.981404	2253.003298	17.864256	-0.045789	2.644704
239.946535	2245.076729	17.869261	-0.045777	2.640472
239.827371	2237.109316	17.874266	-0.045749	2.636205
239.906809	2229.106897	17.879271	-0.045759	2.631925
239.686108	2221.137183	17.884275	-0.045713	2.627637
239.724293	2213.176894	17.889280	-0.045714	2.623363
239.697720	2205.200432	17.894285	-0.045704	2.619070
239.559147	2197.239320	17.899290	-0.045673	2.614770
239.464114	2189.264037	17.904295	-0.045650	2.610458
239.441315	2181.286974	17.909299	-0.045641	2.606143
239.319953	2173.348900	17.914304	-0.045613	2.601836
239.315920	2165.376969	17.919309	-0.045607	2.597510
239.206311	2157.337032	17.924314	-0.045581	2.593134
239.077193	2149.271905	17.929319	-0.045552	2.588735
238.924588	2141.315596	17.934323	-0.045518	2.584386
238.994499	2133.407756	17.939328	-0.045526	2.580072
239.007304	2125.445562	17.944333	-0.045523	2.575716
238.772143	2117.490652	17.949338	-0.045474	2.571340
239.115185	2109.488981	17.954343	-0.045532	2.566971
238.570157	2101.584410	17.959347	-0.045426	2.562587
238.648576	2093.625867	17.964352	-0.045435	2.558208
238.566993	2085.662656	17.969357	-0.045415	2.553808
238.470787	2077.662864	17.974362	-0.045391	2.549380
238.434584	2069.713086	17.979367	-0.045379	2.544975
238.448536	2061.737828	17.984371	-0.045377	2.540552
238.640804	2053.774286	17.989376	-0.045407	2.536141
238.324479	2045.834818	17.994381	-0.045343	2.531699
238.263351	2037.843114	17.999386	-0.045327	2.527239
238.295201	2029.896127	18.004391	-0.045327	2.522802
238.138653	2021.928642	18.009395	-0.045293	2.518332
238.084519	2013.982037	18.014400	-0.045278	2.513874
238.132229	2005.957630	18.019405	-0.045281	2.509371
237.869828	1998.000710	18.024410	-0.045227	2.504875
237.780619	1990.075533	18.029415	-0.045205	2.500402
237.666150	1982.106518	18.034419	-0.045179	2.495895
237.811467	1974.114325	18.039424	-0.045200	2.491385
237.597934	1966.162765	18.044429	-0.045155	2.486863
237.530934	1958.201892	18.049434	-0.045138	2.482339
237.692355	1950.249288	18.054439	-0.045162	2.477828
237.747347	1942.247677	18.059443	-0.045167	2.473273
237.455932	1934.316703	18.064448	-0.045108	2.468724
237.544665	1926.315876	18.069453	-0.045119	2.464155
237.426009	1918.390332	18.074458	-0.045092	2.459606
237.461989	1910.438691	18.079463	-0.045093	2.455044
237.310228	1902.465861	18.084467	-0.045060	2.450448
237.390826	1894.513393	18.089472	-0.045069	2.445872
237.204464	1886.575893	18.094477	-0.045030	2.441276
237.102426	1878.625662	18.099482	-0.045005	2.436670
237.047634	1870.620249	18.104487	-0.044990	2.432028
237.009477	1862.607543	18.109491	-0.044977	2.427373
236.769916	1854.682095	18.114496	-0.044928	2.422745
236.752824	1846.728908	18.119501	-0.044919	2.418109
236.881402	1838.743398	18.124506	-0.044938	2.413456
236.598893	1830.813252	18.129511	-0.044880	2.408795
236.567690	1822.834698	18.134515	-0.044869	2.404116
236.595910	1814.899377	18.139520	-0.044869	2.399458
236.410114	1806.957291	18.144525	-0.044829	2.394770
236.362742	1798.957676	18.149530	-0.044815	2.390049
236.437366	1791.005652	18.154535	-0.044824	2.385357
236.319345	1783.063343	18.159539	-0.044796	2.380647
236.282509	1775.122278	18.164544	-0.044784	2.375934
236.056094	1767.168594	18.169549	-0.044737	2.371189
235.965814	1759.197512	18.174554	-0.044715	2.366435
235.920404	1751.265999	18.179559	-0.044701	2.361699
235.906816	1743.307010	18.184563	-0.044693	2.356939
236.051618	1735.319583	18.189568	-0.044715	2.352166
235.907634	1727.340226	18.194573	-0.044683	2.347364
235.855267	1719.390303	18.199578	-0.044668	2.342577
235.908587	1711.454765	18.204583	-0.044673	2.337798
235.809249	1703.496721	18.209587	-0.044649	2.332984
235.623976	1695.562190	18.214592	-0.044609	2.328166
235.512413	1687.616435	18.219597	-0.044583	2.323337
235.579997	1679.654663	18.224602	-0.044590	2.318504
235.490398	1671.721138	18.229607	-0.044568	2.313664
235.403336	1663.728800	18.234611	-0.044547	2.308779
235.454773	1655.769673	18.239616	-0.044551	2.303915
235.210915	1647.866719	18.244621	-0.044501	2.299051
234.883124	1639.939601	18.249626	-0.044434	2.294154
234.841757	1631.960653	18.254631	-0.044421	2.289239
234.965585	1623.977661	18.259635	-0.044439	2.284325
234.814324	1616.071570	18.264640	-0.044406	2.279425
234.825424	1608.102549	18.269645	-0.044403	2.274489
234.920008	1600.039075	18.274650	-0.044415	2.269490
234.842122	1592.112107	18.279655	-0.044395	2.264551
234.517513	1584.196630	18.284659	-0.044330	2.259587
234.728820	1576.242663	18.289664	-0.044364	2.254634
234.755879	1568.280068	18.294669	-0.044363	2.249648
234.553263	1560.338213	18.299674	-0.044320	2.244645
234.514680	1552.431997	18.304679	-0.044308	2.239667
234.322354	1544.491861	18.309683	-0.044267	2.234644
234.210137	1536.545687	18.314688	-0.044241	2.229612
234.098134	1528.583270	18.319693	-0.044215	2.224558
233.927066	1520.662507	18.324698	-0.044178	2.219514
233.964383	1512.718142	18.329703	-0.044179	2.214462
233.552395	1504.774760	18.334707	-0.044097	2.209359
233.760302	1496.804073	18.339712	-0.044131	2.204283
233.693656	1488.869556	18.344717	-0.044113	2.199193
233.524768	1480.946976	18.349722	-0.044077	2.194089
233.738272	1472.934451	18.354727	-0.044111	2.188951
233.649428	1464.979447	18.359731	-0.044089	2.183810
233.691821	1457.059360	18.364736	-0.044092	2.178691
233.574355	1449.130955	18.369741	-0.044065	2.173541
233.508971	1441.165073	18.374746	-0.044047	2.168358
233.332563	1433.265403	18.379751	-0.044009	2.163196
233.042790	1425.351886	18.384755	-0.043950	2.158002
233.243858	1417.389322	18.389760	-0.043982	2.152809
233.160106	1409.431802	18.394765	-0.043961	2.147580
232.968700	1401.505774	18.399770	-0.043921	2.142349
232.887252	1393.593658	18.404775	-0.043900	2.137125
232.952226	1385.614136	18.409779	-0.043907	2.131857
232.814035	1377.693777	18.414784	-0.043876	2.126596
232.569059	1369.788495	18.419789	-0.043825	2.121321
232.719185	1361.829330	18.424794	-0.043848	2.116036
232.657769	1353.837724	18.429799	-0.043831	2.110695
232.474924	1345.883191	18.434803	-0.043792	2.105354
232.607261	1337.946648	18.439808	-0.043811	2.100041
232.545115	1330.028766	18.444813	-0.043794	2.094709
232.492097	1322.085362	18.449818	-0.043779	2.089347
232.378275	1314.178567	18.454823	-0.043753	2.083990
232.182252	1306.269149	18.459827	-0.043711	2.078609
232.208110	1298.342794	18.464832	-0.043711	2.073225
232.097526	1290.394170	18.469837	-0.043685	2.067798
232.052486	1282.461711	18.474842	-0.043671	2.062374
232.138968	1274.542307	18.479847	-0.043682	2.056958
231.825162	1266.616623	18.484851	-0.043619	2.051483
231.826382	1258.685892	18.489856	-0.043614	2.046022
231.861753	1250.758663	18.494861	-0.043615	2.040552
231.740428	1242.847268	18.499866	-0.043587	2.035062
231.736557	1234.881645	18.504871	-0.043581	2.029532
231.682904	1226.939888	18.509875	-0.043566	2.023998
231.643979	1219.041818	18.514880	-0.043553	2.018481
231.464386	1211.131316	18.519885	-0.043515	2.012925
231.320048	1203.193142	18.524890	-0.043483	2.007339
231.549063	1195.247390	18.529895	-0.043520	2.001770
231.307714	1187.357660	18.534899	-0.043470	1.996176
231.475287	1179.410177	18.539904	-0.043496	1.990569
231.288494	1171.505714	18.544909	-0.043456	1.984938
230.986847	1163.624020	18.549914	-0.043394	1.979296
230.997433	1155.697124	18.554919	-0.043391	1.973639
230.959812	1147.748505	18.559923	-0.043379	1.967944
231.035301	1139.822291	18.564928	-0.043388	1.962261
230.717616	1131.956942	18.569933	-0.043323	1.956563
230.779264	1123.981119	18.574938	-0.043330	1.950810
230.775339	1116.034484	18.579943	-0.043324	1.945054
230.555611	1108.149953	18.584947	-0.043277	1.939302
230.509197	1100.235969	18.589952	-0.043264	1.933530
230.435372	1092.309011	18.594957	-0.043245	1.927729
230.359530	1084.389451	18.599962	-0.043225	1.921915
230.431367	1076.485177	18.604967	-0.043233	1.916112
230.390858	1068.545643	18.609971	-0.043221	1.910252
230.411434	1060.638721	18.614976	-0.043219	1.904405
230.189881	1052.774000	18.619981	-0.043173	1.898544
230.213601	1044.840835	18.624986	-0.043172	1.892642
230.037204	1036.949172	18.629991	-0.043134	1.886729
229.914503	1029.049232	18.634995	-0.043106	1.880798
229.783585	1021.169311	18.640000	-0.043076	1.874862
229.748905	1013.225944	18.645005	-0.043065	1.868871
229.511522	1005.333200	18.650010	-0.043015	1.862875
229.407257	997.454125	18.655015	-0.042991	1.856885
229.260804	989.528965	18.660019	-0.042958	1.850836
229.410747	981.588696	18.665024	-0.042981	1.844791
229.296968	973.718184	18.670029	-0.042954	1.838747
229.019546	965.842774	18.675034	-0.042897	1.832661
229.164582	957.908177	18.680039	-0.042919	1.826559
228.955960	950.020728	18.685043	-0.042875	1.820431
229.145328	942.103667	18.690048	-0.042905	1.814307
229.216345	934.178978	18.695053	-0.042913	1.808141
228.999564	926.320890	18.700058	-0.042868	1.801973
228.885948	918.463775	18.705063	-0.042841	1.795796
228.711801	910.509299	18.710067	-0.042804	1.789513
228.706382	902.615494	18.715072	-0.042797	1.783277
228.714512	894.731626	18.720077	-0.042794	1.777029
228.621131	886.830488	18.725082	-0.042771	1.770733
228.514410	878.968354	18.730087	-0.042746	1.764443
228.335401	871.100644	18.735091	-0.042708	1.758117
228.255835	863.223374	18.740096	-0.042688	1.751774
228.104978	855.332510	18.745101	-0.042654	1.745387
228.267551	847.421404	18.750106	-0.042679	1.739000
228.161829	839.546866	18.755111	-0.042654	1.732585
227.924159	831.687479	18.760115	-0.042605	1.726141
227.734815	823.861063	18.765120	-0.042565	1.719707
227.711958	815.975355	18.770125	-0.042555	1.713221
227.538159	808.078852	18.775130	-0.042517	1.706682
227.668570	800.175889	18.780135	-0.042537	1.700152
227.497516	792.310945	18.785139	-0.042499	1.693590
227.541827	784.408058	18.790144	-0.042503	1.686998
227.460391	776.552126	18.795149	-0.042482	1.680403
227.381981	768.703990	18.800154	-0.042462	1.673789
227.148508	760.854305	18.805159	-0.042414	1.667127
227.119408	752.978573	18.810163	-0.042403	1.660443
227.170529	745.102013	18.815168	-0.042407	1.653742
227.197945	737.220951	18.820173	-0.042407	1.647007
227.081964	729.377093	18.825178	-0.042381	1.640257
227.104977	721.522272	18.830183	-0.042380	1.633489
226.708820	713.651868	18.835187	-0.042301	1.626620
226.628353	705.799883	18.840192	-0.042281	1.619783
226.489247	697.964941	18.845197	-0.042249	1.612923
226.584778	690.065227	18.850202	-0.042262	1.606010
226.582158	682.235973	18.855207	-0.042256	1.599115
226.278997	674.420359	18.860211	-0.042195	1.592160
226.273288	666.560451	18.865216	-0.042188	1.585177
226.319906	658.713413	18.870221	-0.042192	1.578183
226.174606	650.870452	18.875226	-0.042160	1.571133
225.922351	643.068619	18.880231	-0.042108	1.564073
226.102114	635.186418	18.885235	-0.042136	1.556971
226.004528	627.352711	18.890240	-0.042113	1.549840
225.675629	619.562348	18.895245	-0.042046	1.542682
225.546848	611.734369	18.900250	-0.042017	1.535485
225.700715	603.862945	18.905255	-0.042040	1.528256
225.495430	596.054743	18.910259	-0.041997	1.520998
225.345268	588.260927	18.915264	-0.041964	1.513726
225.317128	580.410447	18.920269	-0.041954	1.506385
225.275975	572.594993	18.925274	-0.041941	1.499039
225.214688	564.790898	18.930279	-0.041924	1.491665
225.068749	556.965992	18.935283	-0.041892	1.484220
225.000400	549.173600	18.940288	-0.041874	1.476782
224.855313	541.329667	18.945293	-0.041842	1.469244
224.799063	533.512456	18.950298	-0.041826	1.461707
224.810862	525.714056	18.955303	-0.041823	1.454160
224.732370	517.893108	18.960307	-0.041803	1.446537
224.648626	510.127767	18.965312	-0.041783	1.438927
224.531659	502.341375	18.970317	-0.041756	1.431251
224.295110	494.577003	18.975322	-0.041707	1.423536
224.235645	486.794960	18.980327	-0.041690	1.415790
224.201183	478.987788	18.985331	-0.041679	1.407980
224.116560	471.219309	18.990336	-0.041658	1.400158
224.082861	463.441284	18.995341	-0.041646	1.392290
223.938994	455.652848	19.000346	-0.041615	1.384348
223.917908	447.889983	19.005351	-0.041605	1.376407
223.665185	440.136181	19.010355	-0.041553	1.368391
223.647795	432.376495	19.015360	-0.041545	1.360361
223.679307	424.601111	19.020365	-0.041546	1.352275
223.368645	416.877274	19.025370	-0.041483	1.344136
223.324971	409.130923	19.030375	-0.041469	1.335969
223.359805	401.353512	19.035379	-0.041471	1.327734
223.427048	393.601578	19.040384	-0.041478	1.319480
223.223688	385.816019	19.045389	-0.041435	1.311089
223.013812	378.047020	19.050394	-0.041391	1.302661
222.976053	370.328719	19.055399	-0.041379	1.294264
222.622036	362.637800	19.060403	-0.041308	1.285785
222.708698	354.917673	19.065408	-0.041319	1.277298
222.666904	347.195555	19.070413	-0.041306	1.268729
222.520637	339.498042	19.075418	-0.041274	1.260109
222.542465	331.794658	19.080423	-0.041273	1.251455
222.249018	324.130049	19.085427	-0.041213	1.242725
222.118030	316.460866	19.090432	-0.041184	1.233958
221.947301	308.768649	19.095437	-0.041147	1.225095
221.978498	301.072133	19.100442	-0.041147	1.216202
222.074884	293.358421	19.105447	-0.041160	1.207236
221.757777	285.739445	19.110451	-0.041096	1.198231
221.658322	278.084290	19.115456	-0.041073	1.189160
221.543650	270.439313	19.120461	-0.041046	1.180027
221.466862	262.782329	19.125466	-0.041027	1.170817
221.200908	255.189673	19.130471	-0.040972	1.161573
221.153692	247.530862	19.135475	-0.040958	1.152219
221.251702	239.847018	19.140480	-0.040972	1.142788
221.143223	232.236300	19.145485	-0.040946	1.133326
220.858514	224.653932	19.150490	-0.040888	1.123781
220.836099	217.053945	19.155495	-0.040879	1.114190
220.525542	209.487168	19.160499	-0.040816	1.104494
220.495942	201.900306	19.165504	-0.040806	1.094749
220.475955	194.310099	19.170509	-0.040797	1.084914
220.294781	186.769047	19.175514	-0.040758	1.075017
220.129993	179.220724	19.180519	-0.040723	1.065022
220.016262	171.665874	19.185523	-0.040697	1.054935
220.049124	164.111101	19.190528	-0.040698	1.044785
219.798789	156.629177	19.195533	-0.040646	1.034569
219.732000	149.098340	19.200538	-0.040629	1.024226
219.826244	141.577684	19.205543	-0.040641	1.013831
219.451509	134.132234	19.210547	-0.040567	1.003320
219.272211	126.665163	19.215552	-0.040528	0.992715
219.149875	119.177515	19.220557	-0.040501	0.981979
218.760112	111.774374	19.225562	-0.040423	0.971180
218.664610	104.337059	19.230567	-0.040400	0.960285
218.466498	96.927117	19.235571	-0.040359	0.949279
218.345072	89.523780	19.240576	-0.040331	0.938173
217.747306	82.214535	19.245581	-0.040215	0.926951
217.158984	74.920374	19.250586	-0.040101	0.915616
216.817346	67.581224	19.255591	-0.040032	0.904137
216.391091	60.506645	19.260595	-0.039948	0.892904