Tue Mar 23 10:36:40 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.466921	0.065856	0.000000	0.000040	0.720016

0.616491	0.072022	0.005005	0.000012	0.720080
0.327933	0.119962	0.010010	0.000066	0.720073
0.608325	0.040580	0.015014	0.000014	0.720015
0.650506	-0.023905	0.020019	0.000006	0.719903
0.614881	-0.021238	0.025024	0.000013	0.719895
0.726445	-0.035314	0.030029	-0.000007	0.719906
0.685135	-0.033258	0.035034	0.000000	0.719896
0.610354	-0.018510	0.040038	0.000014	0.719899
0.604012	-0.015553	0.045043	0.000016	0.719902
0.681382	-0.032688	0.050048	0.000001	0.719895
0.716506	-0.032046	0.055053	-0.000005	0.719909
0.639885	-0.022870	0.060058	0.000009	0.719900
0.605477	-0.016064	0.065062	0.000016	0.719901
0.498884	0.003635	0.070067	0.000036	0.719902
0.524082	-0.003854	0.075072	0.000031	0.719896
0.653642	-0.105977	0.080077	0.000007	0.719740
0.508132	-0.149211	0.085082	0.000034	0.719603
0.510107	-0.147933	0.090086	0.000034	0.719606
0.447857	-0.136407	0.095091	0.000046	0.719607
0.366162	-0.126049	0.100096	0.000061	0.719599
0.673013	-0.175059	0.105101	0.000004	0.719610
0.419953	-0.135257	0.110106	0.000051	0.719599
0.528922	-0.297541	0.115110	0.000031	0.719317
0.679799	-0.347108	0.120115	0.000003	0.719272
0.545310	-0.326990	0.125120	0.000028	0.719264
0.518194	-0.316775	0.130125	0.000033	0.719275
0.571528	-0.329786	0.135130	0.000023	0.719268
0.457764	-0.446887	0.140134	0.000045	0.718997
0.554124	-0.480923	0.145139	0.000027	0.718963
0.481307	-0.471272	0.150144	0.000041	0.718956
0.604296	-0.488024	0.155149	0.000018	0.718966
0.346236	-0.544823	0.160154	0.000066	0.718763
0.421145	-0.617725	0.165158	0.000052	0.718646
0.512750	-0.633674	0.170163	0.000035	0.718646
0.281901	-0.594299	0.175168	0.000078	0.718643
0.284814	-0.706531	0.180173	0.000078	0.718422
0.403999	-0.764770	0.185178	0.000056	0.718348
0.451575	-0.769837	0.190182	0.000047	0.718355
0.413580	-0.818768	0.195187	0.000054	0.718245
0.391689	-0.931853	0.200192	0.000058	0.718013
0.341214	-0.917131	0.205197	0.000068	0.718025
0.273925	-0.934956	0.210202	0.000081	0.717966
0.400378	-1.090636	0.215206	0.000057	0.717702
0.569235	-1.120857	0.220211	0.000026	0.717702
0.431865	-1.139371	0.225216	0.000052	0.717616
0.335928	-1.241179	0.230221	0.000070	0.717381
0.322418	-1.240383	0.235226	0.000072	0.717378
0.352626	-1.320674	0.240230	0.000067	0.717229
0.183225	-1.360748	0.245235	0.000098	0.717090
0.161559	-1.361299	0.250240	0.000103	0.717081
0.163196	-1.494548	0.255245	0.000102	0.716818
0.152153	-1.526714	0.260250	0.000105	0.716750
0.086965	-1.556171	0.265254	0.000117	0.716669
0.212945	-1.687098	0.270259	0.000094	0.716454
0.178988	-1.685614	0.275264	0.000100	0.716445
0.152419	-1.814981	0.280269	0.000105	0.716179
0.149718	-1.839150	0.285274	0.000106	0.716130
0.191487	-1.915266	0.290278	0.000098	0.715993
0.247551	-1.980055	0.295283	0.000088	0.715885
0.129096	-2.020171	0.300288	0.000110	0.715763
0.077120	-2.117417	0.305293	0.000120	0.715552
-0.039807	-2.129758	0.310298	0.000142	0.715486
-0.256751	-2.218507	0.315302	0.000182	0.715233
-0.203182	-2.230322	0.320307	0.000172	0.715228
-0.124680	-2.407233	0.325312	0.000158	0.714905
-0.380513	-2.356389	0.330317	0.000206	0.714915
-2.691736	-2.088391	0.335322	0.000636	0.714630
-3.455650	-1.962534	0.340326	0.000778	0.714609
-3.925255	-1.876011	0.345331	0.000866	0.714615
-3.202629	-2.116981	0.350336	0.000731	0.714392
-4.646163	-1.913783	0.355341	0.001000	0.714284
-4.655541	-1.915444	0.360346	0.001002	0.714277
-4.168838	-2.002955	0.365350	0.000911	0.714276
-4.809936	-2.017922	0.370355	0.001031	0.714019
-5.570876	-1.910011	0.375360	0.001173	0.713964
-5.117618	-1.984656	0.380365	0.001088	0.713976
-5.050675	-1.999047	0.385370	0.001076	0.713971
-5.482446	-2.037110	0.390374	0.001156	0.713742
-6.131990	-1.963001	0.395379	0.001277	0.713659
-6.107785	-1.971386	0.400384	0.001273	0.713651
-5.918543	-2.003087	0.405389	0.001238	0.713654
-6.302857	-1.959226	0.410394	0.001309	0.713605
-6.675798	-2.016453	0.415398	0.001379	0.713359
-6.858705	-1.982255	0.420403	0.001413	0.713362
-7.562521	-1.859854	0.425408	0.001544	0.713356
-6.798063	-1.991630	0.430413	0.001402	0.713365
-6.566642	-2.072857	0.435418	0.001359	0.713285
-8.041936	-1.940358	0.440422	0.001634	0.713025
-7.742415	-1.991864	0.445427	0.001578	0.713029
-8.011646	-1.948287	0.450432	0.001628	0.713020
-8.125074	-1.923682	0.455437	0.001650	0.713029
-7.897264	-1.966021	0.460442	0.001607	0.713025
-8.137317	-2.031919	0.465446	0.001652	0.712808
-8.797312	-1.963133	0.470451	0.001775	0.712711
-9.106739	-1.911529	0.475456	0.001833	0.712704
-8.888121	-1.944667	0.480461	0.001792	0.712715
-8.865265	-1.953042	0.485466	0.001788	0.712707
-9.102097	-1.908924	0.490470	0.001832	0.712710
-8.925303	-2.032182	0.495475	0.001799	0.712527
-9.891851	-1.931717	0.500480	0.001979	0.712384
-9.479787	-2.002258	0.505485	0.001903	0.712390
-9.771155	-1.953125	0.510490	0.001957	0.712384
-10.199726	-1.875436	0.515494	0.002037	0.712387
-9.622971	-1.975670	0.520499	0.001930	0.712391
-10.062164	-1.937412	0.525504	0.002011	0.712312
-10.758350	-1.920718	0.530509	0.002141	0.712097
-10.144120	-2.033582	0.535514	0.002027	0.712090
-10.806637	-1.916172	0.540518	0.002150	0.712089
-10.604477	-1.948578	0.545523	0.002113	0.712096
-10.479442	-1.975348	0.550528	0.002090	0.712087
-10.455362	-1.973913	0.555533	0.002085	0.712098
-11.285445	-1.987108	0.560538	0.002240	0.711777
-11.638918	-1.929997	0.565542	0.002306	0.711765
-11.577799	-1.940252	0.570547	0.002295	0.711766
-11.693139	-1.924196	0.575552	0.002316	0.711757
-11.464970	-1.961551	0.580557	0.002274	0.711763
-11.379248	-1.978224	0.585562	0.002258	0.711760
-11.473416	-1.993137	0.590566	0.002275	0.711697
-12.351709	-1.956063	0.595571	0.002439	0.711459
-12.105694	-2.004345	0.600576	0.002393	0.711450
-12.503258	-1.930417	0.605581	0.002467	0.711456
-12.554726	-1.924173	0.610586	0.002477	0.711450
-12.452755	-1.939595	0.615590	0.002458	0.711455
-12.187033	-1.984620	0.620595	0.002409	0.711459
-12.516095	-2.010979	0.625600	0.002470	0.711290
-13.507939	-1.907308	0.630605	0.002655	0.711144
-13.124618	-1.979074	0.635610	0.002584	0.711137
-13.631057	-1.887898	0.640614	0.002678	0.711138
-13.605663	-1.890577	0.645619	0.002673	0.711142
-13.203382	-1.965760	0.650624	0.002599	0.711135
-13.106633	-1.978102	0.655629	0.002581	0.711144
-13.594275	-1.942157	0.660634	0.002672	0.711042
-14.239495	-1.913501	0.665638	0.002792	0.710870
-13.498390	-2.040999	0.670643	0.002654	0.710879
-14.180930	-1.924114	0.675648	0.002781	0.710869
-14.129460	-1.927688	0.680653	0.002772	0.710880
-14.149176	-1.927450	0.685658	0.002775	0.710873
-14.238153	-1.911824	0.690662	0.002792	0.710873
-14.412712	-1.991852	0.695667	0.002825	0.710651
-15.361857	-1.883172	0.700672	0.003001	0.710530
-14.887482	-1.961864	0.705677	0.002913	0.710541
-14.940656	-1.955429	0.710682	0.002923	0.710535
-15.374705	-1.878828	0.715686	0.003004	0.710533
-14.624511	-2.008928	0.720691	0.002865	0.710540
-15.014734	-1.942128	0.725696	0.002937	0.710535
-15.597607	-1.956145	0.730701	0.003046	0.710299
-15.927262	-1.936449	0.735706	0.003107	0.710221
-15.737378	-1.971094	0.740710	0.003072	0.710219
-15.823223	-1.952979	0.745715	0.003088	0.710224
-16.247137	-1.881657	0.750720	0.003167	0.710216
-15.622348	-1.988442	0.755725	0.003051	0.710225
-15.890200	-1.942896	0.760730	0.003101	0.710220
-16.543474	-1.957738	0.765734	0.003223	0.709958
-16.774679	-1.945650	0.770739	0.003266	0.709899
-17.089748	-1.892314	0.775744	0.003325	0.709894
-16.969857	-1.910897	0.780749	0.003302	0.709899
-16.708120	-1.959710	0.785754	0.003254	0.709894
-16.607651	-1.978502	0.790758	0.003235	0.709892
-16.801809	-1.941128	0.795763	0.003271	0.709898
-17.189309	-1.968499	0.800768	0.003344	0.709705
-17.736202	-1.923322	0.805773	0.003445	0.709600
-17.793521	-1.915091	0.810778	0.003456	0.709596
-17.797402	-1.915522	0.815782	0.003457	0.709593
-17.606694	-1.946062	0.820787	0.003422	0.709600
-17.906687	-1.895487	0.825792	0.003478	0.709594
-18.012701	-1.872727	0.830797	0.003497	0.709602
-17.848483	-1.953900	0.835802	0.003467	0.709498
-18.678837	-1.921291	0.840806	0.003622	0.709267
-18.501479	-1.949376	0.845811	0.003589	0.709274
-19.122645	-1.842115	0.850816	0.003704	0.709267
-18.663076	-1.920643	0.855821	0.003619	0.709273
-18.587341	-1.937679	0.860826	0.003605	0.709266
-19.130020	-1.841635	0.865830	0.003706	0.709264
-18.520641	-1.947559	0.870835	0.003593	0.709270
-19.392763	-1.944688	0.875840	0.003755	0.708964
-19.820000	-1.871824	0.880845	0.003835	0.708957
-19.862655	-1.866358	0.885850	0.003843	0.708953
-19.282610	-1.968267	0.890854	0.003735	0.708956
-19.458059	-1.935242	0.895859	0.003768	0.708959
-19.925735	-1.855522	0.900864	0.003855	0.708952
-19.404500	-1.944652	0.905869	0.003758	0.708959
-19.849966	-1.963193	0.910874	0.003841	0.708763
-21.216803	-1.782656	0.915878	0.004095	0.708636
-20.452643	-1.915156	0.920883	0.003953	0.708643
-20.543867	-1.904034	0.925888	0.003970	0.708633
-20.724904	-1.866079	0.930893	0.004004	0.708644
-20.697751	-1.873675	0.935898	0.003999	0.708638
-20.749762	-1.865411	0.940902	0.004009	0.708636
-20.464901	-1.915541	0.945907	0.003956	0.708637
-21.213387	-1.924505	0.950912	0.004095	0.708352
-21.460373	-1.878927	0.955917	0.004142	0.708355
-21.596155	-1.857176	0.960922	0.004167	0.708350
-21.456389	-1.882035	0.965926	0.004141	0.708350
-21.044954	-1.952735	0.970931	0.004065	0.708355
-21.388598	-1.896085	0.975936	0.004129	0.708345
-21.457367	-1.884834	0.980941	0.004141	0.708343
-22.359974	-1.890282	0.985946	0.004310	0.708010
-22.398125	-1.883281	0.990950	0.004317	0.708010
-22.301724	-1.895431	0.995955	0.004299	0.708020
-22.636515	-1.840744	1.000960	0.004361	0.708010
-22.557010	-1.851634	1.005965	0.004347	0.708016
-22.443580	-1.873747	1.010970	0.004326	0.708012
-22.491426	-1.866380	1.015974	0.004335	0.708010
-22.519326	-1.917671	1.020979	0.004340	0.707897
-23.689423	-1.810457	1.025984	0.004558	0.707693
-23.209361	-1.890670	1.030989	0.004469	0.707704
-23.535536	-1.835102	1.035994	0.004529	0.707698
-23.645893	-1.815155	1.040998	0.004550	0.707699
-23.185407	-1.894486	1.046003	0.004464	0.707704
-23.704863	-1.806419	1.051008	0.004561	0.707695
-23.480902	-1.840837	1.056013	0.004520	0.707706
-23.583563	-1.935251	1.061018	0.004539	0.707479
-24.758129	-1.775540	1.066022	0.004757	0.707380
-24.313722	-1.850336	1.071027	0.004675	0.707388
-24.286303	-1.861125	1.076032	0.004670	0.707376
-24.452240	-1.828745	1.081037	0.004701	0.707382
-24.477645	-1.827592	1.086042	0.004706	0.707375
-24.407391	-1.839131	1.091046	0.004693	0.707377
-24.080028	-1.924524	1.096051	0.004632	0.707322
-25.130981	-1.857298	1.101056	0.004828	0.707081
-25.138812	-1.853834	1.106061	0.004829	0.707085
-25.073502	-1.866864	1.111066	0.004817	0.707082
-25.256673	-1.836816	1.116070	0.004851	0.707076
-24.838832	-1.906571	1.121075	0.004774	0.707086
-25.248704	-1.838997	1.126080	0.004850	0.707075
-25.141254	-1.905122	1.131085	0.004830	0.706980
-25.912064	-1.882591	1.136090	0.004974	0.706749
-25.909968	-1.883111	1.141094	0.004973	0.706749
-26.031687	-1.857642	1.146099	0.004996	0.706756
-26.411535	-1.794988	1.151104	0.005067	0.706746
-26.041686	-1.858407	1.156109	0.004998	0.706751
-25.769647	-1.908280	1.161114	0.004948	0.706748
-26.093765	-1.886632	1.166118	0.005008	0.706675
-26.736708	-1.883418	1.171123	0.005128	0.706451
-26.702791	-1.893958	1.176128	0.005122	0.706442
-27.077938	-1.824411	1.181133	0.005192	0.706447
-26.976769	-1.842006	1.186138	0.005173	0.706448
-27.084470	-1.824705	1.191142	0.005193	0.706444
-26.962019	-1.841162	1.196147	0.005170	0.706454
-27.023673	-1.839950	1.201152	0.005182	0.706434
-27.355565	-1.931409	1.206157	0.005244	0.706132
-27.540095	-1.900531	1.211162	0.005278	0.706127
-27.924958	-1.832861	1.216166	0.005350	0.706125
-27.493920	-1.906337	1.221171	0.005270	0.706132
-27.790870	-1.857751	1.226176	0.005325	0.706123
-27.794538	-1.856235	1.231181	0.005326	0.706124
-27.457717	-1.962089	1.236186	0.005263	0.706032
-28.673823	-1.833721	1.241190	0.005490	0.705854
-28.152845	-1.921679	1.246195	0.005393	0.705864
-28.592680	-1.847701	1.251200	0.005475	0.705855
-28.641456	-1.834926	1.256205	0.005484	0.705863
-28.151648	-1.922448	1.261210	0.005393	0.705862
-28.544088	-1.855094	1.266214	0.005466	0.705857
-28.833495	-1.933946	1.271219	0.005520	0.705594
-29.436185	-1.864209	1.276224	0.005632	0.705518
-29.329097	-1.880108	1.281229	0.005613	0.705524
-29.181019	-1.905639	1.286234	0.005585	0.705526
-29.391993	-1.869734	1.291238	0.005624	0.705522
-28.991148	-1.939812	1.296243	0.005550	0.705525
-29.232643	-1.946158	1.301248	0.005595	0.705425
-30.274976	-1.866309	1.306253	0.005789	0.705212
-29.799786	-1.951346	1.311258	0.005701	0.705211
-30.285560	-1.868203	1.316262	0.005791	0.705204
-30.249198	-1.871071	1.321267	0.005785	0.705211
-29.968120	-1.923797	1.326272	0.005732	0.705206
-30.040742	-1.907318	1.331277	0.005746	0.705213
-30.348723	-1.967738	1.336282	0.005803	0.704980
-31.227264	-1.857937	1.341286	0.005967	0.704886
-30.926830	-1.908379	1.346291	0.005911	0.704892
-30.956308	-1.907455	1.351296	0.005917	0.704883
-31.340424	-1.836114	1.356301	0.005988	0.704888
-31.101640	-1.879442	1.361306	0.005944	0.704887
-31.032517	-1.894582	1.366310	0.005931	0.704881
-31.222971	-1.971285	1.371315	0.005967	0.704658
-32.049796	-1.859756	1.376320	0.006121	0.704585
-31.932456	-1.877255	1.381325	0.006099	0.704592
-31.697575	-1.919733	1.386330	0.006055	0.704591
-32.325790	-1.809374	1.391334	0.006172	0.704587
-31.935975	-1.876331	1.396339	0.006100	0.704592
-31.931287	-1.880914	1.401344	0.006099	0.704584
-32.449541	-1.921084	1.406349	0.006196	0.704317
-33.080407	-1.836530	1.411354	0.006313	0.704261
-32.802610	-1.888322	1.416358	0.006262	0.704256
-32.882808	-1.871502	1.421363	0.006277	0.704261
-33.260300	-1.808230	1.426368	0.006347	0.704252
-32.953859	-1.859826	1.431373	0.006290	0.704258
-32.832426	-1.880070	1.436378	0.006268	0.704261
-33.237252	-1.871522	1.441382	0.006343	0.704133
-33.853500	-1.849144	1.446387	0.006458	0.703956
-33.580367	-1.901845	1.451392	0.006407	0.703948
-34.000771	-1.823726	1.456397	0.006486	0.703954
-33.639154	-1.889221	1.461402	0.006418	0.703952
-33.632615	-1.893241	1.466406	0.006417	0.703946
-33.784342	-1.863091	1.471411	0.006446	0.703952
-34.127433	-1.858516	1.476416	0.006509	0.703837
-34.630504	-1.868993	1.481421	0.006603	0.703635
-34.282988	-1.931860	1.486426	0.006539	0.703633
-35.069419	-1.794023	1.491430	0.006685	0.703628
-34.582966	-1.877519	1.496435	0.006595	0.703635
-34.517187	-1.891517	1.501440	0.006583	0.703630
-34.815239	-1.835749	1.506445	0.006638	0.703635
-34.734371	-1.889670	1.511450	0.006623	0.703555
-35.348407	-1.889484	1.516454	0.006738	0.703334
-35.406258	-1.875297	1.521459	0.006748	0.703342
-35.786725	-1.812490	1.526464	0.006819	0.703332
-35.583669	-1.844620	1.531469	0.006782	0.703340
-35.518294	-1.856458	1.536474	0.006770	0.703339
-35.983184	-1.776244	1.541478	0.006856	0.703333
-35.480930	-1.875624	1.546483	0.006763	0.703313
-36.197996	-1.904818	1.551488	0.006896	0.702996
-36.511815	-1.844887	1.556493	0.006955	0.703004
-36.522624	-1.842874	1.561498	0.006957	0.703004
-36.528525	-1.844208	1.566502	0.006958	0.702999
-36.580334	-1.831023	1.571507	0.006968	0.703007
-36.815103	-1.793335	1.576512	0.007012	0.702998
-36.463293	-1.852681	1.581517	0.006946	0.703005
-36.624740	-1.947796	1.586522	0.006977	0.702754
-37.742296	-1.783275	1.591526	0.007185	0.702684
-37.569214	-1.808909	1.596531	0.007152	0.702694
-37.334939	-1.855259	1.601536	0.007109	0.702685
-37.443321	-1.832299	1.606541	0.007129	0.702692
-37.376016	-1.843632	1.611546	0.007117	0.702693
-37.590750	-1.807814	1.616550	0.007157	0.702688
-37.389336	-1.923668	1.621555	0.007120	0.702526
-38.502559	-1.803209	1.626560	0.007327	0.702368
-38.128728	-1.868493	1.631565	0.007257	0.702371
-38.159863	-1.862934	1.636570	0.007263	0.702371
-38.603505	-1.786768	1.641574	0.007346	0.702365
-37.997270	-1.889085	1.646579	0.007233	0.702376
-38.164963	-1.863078	1.651584	0.007264	0.702368
-38.511729	-1.888422	1.656589	0.007329	0.702192
-39.363344	-1.793882	1.661594	0.007488	0.702076
-39.062131	-1.850542	1.666598	0.007432	0.702069
-38.641224	-1.918859	1.671603	0.007354	0.702083
-39.465282	-1.778382	1.676608	0.007507	0.702070
-39.131224	-1.834919	1.681613	0.007445	0.702076
-38.837883	-1.888055	1.686618	0.007390	0.702074
-39.426200	-1.890157	1.691622	0.007500	0.701857
-40.163551	-1.812524	1.696627	0.007637	0.701748
-39.809093	-1.880759	1.701632	0.007571	0.701738
-39.793253	-1.880065	1.706637	0.007569	0.701745
-40.004230	-1.842713	1.711642	0.007608	0.701744
-39.800603	-1.880742	1.716646	0.007570	0.701740
-39.550532	-1.921846	1.721651	0.007524	0.701747
-40.613101	-1.888407	1.726656	0.007722	0.701431
-40.679097	-1.873317	1.731661	0.007734	0.701438
-40.621859	-1.881509	1.736666	0.007723	0.701441
-40.864937	-1.841708	1.741670	0.007769	0.701434
-40.855140	-1.838243	1.746675	0.007767	0.701445
-40.845172	-1.844174	1.751680	0.007765	0.701436
-40.468557	-1.945956	1.756685	0.007695	0.701366
-41.468261	-1.887808	1.761690	0.007881	0.701122
-41.674282	-1.851645	1.766694	0.007920	0.701121
-41.597515	-1.863089	1.771699	0.007906	0.701125
-41.583660	-1.868208	1.776704	0.007903	0.701120
-41.411172	-1.896101	1.781709	0.007871	0.701125
-41.301305	-1.916604	1.786714	0.007851	0.701123
-41.802315	-1.907888	1.791718	0.007944	0.700960
-42.407927	-1.841456	1.796723	0.008057	0.700875
-41.932526	-1.929711	1.801728	0.007969	0.700868
-42.033680	-1.908895	1.806733	0.007988	0.700874
-42.359003	-1.849882	1.811738	0.008048	0.700875
-42.450770	-1.837093	1.816742	0.008065	0.700868
-41.997718	-1.967916	1.821747	0.007981	0.700766
-43.292351	-1.853220	1.826752	0.008222	0.700531
-43.029442	-1.899278	1.831757	0.008173	0.700532
-42.952247	-1.911493	1.836762	0.008159	0.700535
-43.126166	-1.883477	1.841766	0.008192	0.700529
-42.811810	-1.933397	1.846771	0.008133	0.700541
-43.194387	-1.872988	1.851776	0.008205	0.700525
-43.625796	-1.933164	1.856781	0.008285	0.700247
-44.159226	-1.849624	1.861786	0.008384	0.700223
-44.354732	-1.820065	1.866790	0.008421	0.700212
-43.773389	-1.918247	1.871795	0.008313	0.700223
-44.074085	-1.868663	1.876800	0.008369	0.700215
-44.326224	-1.822504	1.881805	0.008416	0.700217
-43.778722	-1.919346	1.886810	0.008314	0.700219
-44.418991	-1.966020	1.891814	0.008433	0.699892
-44.755723	-1.899664	1.896819	0.008496	0.699905
-44.982693	-1.864414	1.901824	0.008538	0.699894
-44.686022	-1.915688	1.906829	0.008483	0.699897
-44.842098	-1.886388	1.911834	0.008512	0.699900
-45.359666	-1.796901	1.916838	0.008609	0.699894
-44.602788	-1.975871	1.921843	0.008468	0.699805
-45.825830	-1.860499	1.926848	0.008696	0.699596
-45.973979	-1.831767	1.931853	0.008723	0.699600
-45.682816	-1.883098	1.936858	0.008669	0.699601
-45.861853	-1.854202	1.941862	0.008703	0.699595
-45.792858	-1.862805	1.946867	0.008690	0.699602
-45.907455	-1.846782	1.951872	0.008711	0.699593
-45.455056	-1.987430	1.956877	0.008627	0.699471
-46.568475	-1.887861	1.961882	0.008835	0.699270
-46.632461	-1.879899	1.966886	0.008847	0.699263
-46.288218	-1.935856	1.971891	0.008783	0.699274
-46.777094	-1.853169	1.976896	0.008874	0.699264
-46.911703	-1.827083	1.981901	0.008899	0.699268
-46.711868	-1.861439	1.986906	0.008862	0.699271
-46.542406	-1.971619	1.991910	0.008830	0.699108
-47.443321	-1.880510	1.996915	0.008998	0.698967
-47.358564	-1.899245	2.001920	0.008983	0.698959

-47.516306	-1.871752	2.011917	0.009012	0.698958
-47.415264	-1.887598	2.021914	0.008994	0.698962
-47.404947	-1.889650	2.031910	0.008992	0.698961
-47.582492	-1.935819	2.041907	0.009025	0.698802
-48.061541	-1.892004	2.051904	0.009114	0.698717
-48.003996	-1.865234	2.061901	0.009104	0.698792
-47.402425	-1.914171	2.071898	0.008992	0.698911
-47.189425	-1.926145	2.081894	0.008953	0.698963
-47.344312	-1.899546	2.091891	0.008982	0.698961
-47.470266	-1.878144	2.101888	0.009005	0.698958
-47.358277	-1.898249	2.111885	0.008985	0.698957
-47.110612	-1.940202	2.121882	0.008939	0.698962
-47.336611	-1.901115	2.131878	0.008981	0.698959
-47.447098	-1.880934	2.141875	0.009002	0.698959
-47.300701	-1.847768	2.151872	0.008974	0.699080
-46.397549	-1.917338	2.161869	0.008807	0.699265
-46.482368	-1.900965	2.171866	0.008823	0.699267
-46.693408	-1.861816	2.181862	0.008862	0.699270
-46.423767	-1.911378	2.191859	0.008812	0.699267
-46.119894	-1.820308	2.201856	0.008755	0.699561
-45.743273	-1.869742	2.211853	0.008686	0.699597
-45.506773	-1.910662	2.221850	0.008642	0.699599
-45.821083	-1.852484	2.231846	0.008700	0.699603
-45.054273	-1.844769	2.241843	0.008558	0.699896
-44.920005	-1.868846	2.251840	0.008533	0.699895
-44.823078	-1.885571	2.261837	0.008515	0.699896
-44.754611	-1.841006	2.271834	0.008503	0.700011
-43.843604	-1.898896	2.281830	0.008333	0.700223
-43.853291	-1.898345	2.291827	0.008335	0.700220
-44.192251	-1.836851	2.301824	0.008398	0.700222
-43.387783	-1.880411	2.311821	0.008249	0.700424
-43.030029	-1.886801	2.321818	0.008182	0.700540
-43.122445	-1.871347	2.331814	0.008200	0.700538
-42.869493	-1.917200	2.341811	0.008153	0.700536
-42.470767	-1.836939	2.351808	0.008079	0.700842
-41.906247	-1.922148	2.361805	0.007974	0.700873
-41.948333	-1.913470	2.371802	0.007982	0.700875
-42.173791	-1.852742	2.381798	0.008024	0.700917
-41.321121	-1.902046	2.391795	0.007865	0.701125
-41.472358	-1.874448	2.401792	0.007894	0.701125
-41.231091	-1.917137	2.411789	0.007849	0.701126
-40.940614	-1.854599	2.421786	0.007795	0.701357
-40.477571	-1.895037	2.431782	0.007709	0.701442
-40.539799	-1.883770	2.441779	0.007721	0.701442
-40.522122	-1.830211	2.451776	0.007718	0.701556
-39.550807	-1.909907	2.461773	0.007537	0.701745
-39.762351	-1.872098	2.471770	0.007577	0.701745
-39.669909	-1.883503	2.481766	0.007560	0.701755
-39.067428	-1.832720	2.491763	0.007448	0.702075
-38.880179	-1.868016	2.501760	0.007413	0.702071
-38.666847	-1.903636	2.511757	0.007373	0.702075
-38.441686	-1.853902	2.521754	0.007332	0.702257
-37.816991	-1.908567	2.531750	0.007215	0.702371
-38.064660	-1.864126	2.541747	0.007262	0.702371
-37.872217	-1.873026	2.551744	0.007226	0.702422
-37.092157	-1.879371	2.561741	0.007081	0.702690
-37.154850	-1.866322	2.571738	0.007093	0.702694
-36.789421	-1.931566	2.581734	0.007025	0.702693
-36.630828	-1.854913	2.591731	0.006996	0.702905
-36.209141	-1.881761	2.601728	0.006917	0.703002
-36.182829	-1.885661	2.611725	0.006913	0.703003
-36.228017	-1.832136	2.621722	0.006921	0.703095
-35.117081	-1.905685	2.631718	0.006715	0.703346
-35.228549	-1.886300	2.641715	0.006735	0.703345
-35.261117	-1.881097	2.651712	0.006742	0.703343
-34.844079	-1.861252	2.661709	0.006664	0.703533
-34.708785	-1.832934	2.671706	0.006639	0.703638
-34.311133	-1.902911	2.681702	0.006565	0.703640
-34.332859	-1.859528	2.691699	0.006570	0.703719
-33.507173	-1.890859	2.701696	0.006416	0.703953
-33.573414	-1.879654	2.711693	0.006429	0.703951
-33.707335	-1.854990	2.721690	0.006454	0.703952
-32.952946	-1.867680	2.731686	0.006313	0.704198
-32.996145	-1.829505	2.741683	0.006322	0.704259
-32.769540	-1.869803	2.751680	0.006280	0.704259
-32.533428	-1.832731	2.761677	0.006236	0.704418
-31.737404	-1.886332	2.771674	0.006088	0.704596
-31.812748	-1.873118	2.781670	0.006102	0.704595
-31.757023	-1.884701	2.791667	0.006092	0.704591
-31.029100	-1.883166	2.801664	0.005956	0.704855
-31.068325	-1.859828	2.811661	0.005964	0.704888
-30.807009	-1.904720	2.821658	0.005915	0.704891
-30.687298	-1.873168	2.831654	0.005893	0.704997
-30.145903	-1.860385	2.841651	0.005793	0.705217
-30.062721	-1.875583	2.851648	0.005777	0.705216
-30.183636	-1.854752	2.861645	0.005800	0.705214
-29.355648	-1.869100	2.871642	0.005646	0.705482
-29.363863	-1.843432	2.881638	0.005648	0.705530
-29.272318	-1.860585	2.891635	0.005631	0.705528
-29.050155	-1.822700	2.901632	0.005590	0.705684
-28.428555	-1.845696	2.911629	0.005474	0.705860
-28.370194	-1.853556	2.921626	0.005463	0.705865
-28.343173	-1.852101	2.931622	0.005459	0.705877
-27.836176	-1.816252	2.941619	0.005364	0.706131
-27.447113	-1.885927	2.951616	0.005292	0.706130
-27.724959	-1.836663	2.961613	0.005344	0.706129
-26.989557	-1.856323	2.971610	0.005207	0.706353
-26.744834	-1.852299	2.981606	0.005162	0.706448
-26.764131	-1.849116	2.991603	0.005166	0.706447
-26.778242	-1.790518	3.001600	0.005168	0.706560
-25.977074	-1.836216	3.011597	0.005019	0.706754
-25.616885	-1.899458	3.021594	0.004953	0.706756
-25.957172	-1.839107	3.031590	0.005016	0.706755
-25.030835	-1.843891	3.041587	0.004844	0.707077
-24.920792	-1.858972	3.051584	0.004824	0.707085
-24.840191	-1.874759	3.061581	0.004809	0.707082
-24.933771	-1.803892	3.071578	0.004826	0.707191
-24.072558	-1.862062	3.081574	0.004666	0.707382
-24.147470	-1.848501	3.091571	0.004680	0.707382
-24.079609	-1.859255	3.101568	0.004668	0.707384
-23.458284	-1.809409	3.111565	0.004552	0.707706
-23.123422	-1.869963	3.121562	0.004490	0.707704
-23.367262	-1.826104	3.131558	0.004536	0.707704
-22.885412	-1.816630	3.141555	0.004446	0.707895
-22.514317	-1.823557	3.151552	0.004377	0.708014
-22.429869	-1.838707	3.161549	0.004362	0.708013
-22.174087	-1.857538	3.171546	0.004314	0.708066
-21.477754	-1.838085	3.181542	0.004185	0.708354
-21.361414	-1.858021	3.191539	0.004163	0.708355
-21.524009	-1.831604	3.201536	0.004194	0.708350
-21.228677	-1.808064	3.211533	0.004139	0.708502
-20.474530	-1.871609	3.221530	0.003999	0.708643
-20.818796	-1.809778	3.231526	0.004063	0.708644
-20.434530	-1.862556	3.241523	0.003992	0.708675
-20.068789	-1.782655	3.251520	0.003924	0.708965
-19.600503	-1.869947	3.261517	0.003837	0.708957
-19.572301	-1.873279	3.271514	0.003832	0.708960
-19.389995	-1.810713	3.281510	0.003798	0.709150
-18.579330	-1.896241	3.291507	0.003647	0.709268
-18.824216	-1.852550	3.301504	0.003693	0.709268
-18.721345	-1.872778	3.311501	0.003674	0.709264
-18.029713	-1.832029	3.321498	0.003545	0.709592
-18.008030	-1.830604	3.331494	0.003541	0.709602
-17.617105	-1.900948	3.341491	0.003469	0.709600
-17.750934	-1.830367	3.351488	0.003494	0.709693
-16.894218	-1.880517	3.361485	0.003335	0.709898
-17.045457	-1.852420	3.371482	0.003363	0.709900
-17.091495	-1.844397	3.381478	0.003372	0.709899
-16.158490	-1.878593	3.391475	0.003198	0.710163
-16.217154	-1.840251	3.401472	0.003209	0.710218
-15.866552	-1.901727	3.411469	0.003144	0.710220
-15.957090	-1.866344	3.421466	0.003161	0.710258
-15.275629	-1.848176	3.431462	0.003034	0.710537
-15.023619	-1.893101	3.441459	0.002988	0.710536
-15.321762	-1.839065	3.451456	0.003043	0.710538
-14.803362	-1.839444	3.461453	0.002947	0.710721
-14.325651	-1.848396	3.471450	0.002858	0.710873
-14.359428	-1.841501	3.481446	0.002865	0.710874
-14.215483	-1.866741	3.491443	0.002838	0.710875
-13.826250	-1.804050	3.501440	0.002766	0.711138
-13.540754	-1.853060	3.511437	0.002713	0.711141
-13.516107	-1.857279	3.521434	0.002708	0.711141
-12.989564	-1.846883	3.531430	0.002611	0.711349
-12.699317	-1.845080	3.541427	0.002557	0.711455
-12.885627	-1.811715	3.551424	0.002592	0.711455
-12.513204	-1.828030	3.561421	0.002522	0.711555
-11.892388	-1.834246	3.571418	0.002407	0.711763
-11.802424	-1.849396	3.581414	0.002390	0.711764
-11.866128	-1.837679	3.591411	0.002402	0.711765
-11.129041	-1.812282	3.601408	0.002265	0.712077
-10.728681	-1.876496	3.611405	0.002191	0.712091
-10.377229	-1.937367	3.621402	0.002126	0.712094
-10.322703	-1.944988	3.631398	0.002116	0.712098
-9.861604	-1.884972	3.641395	0.002030	0.712381
-9.692532	-1.909037	3.651392	0.001999	0.712392
-9.461043	-1.949202	3.661389	0.001956	0.712394
-9.676565	-1.902752	3.671386	0.001996	0.712410
-8.452954	-1.967519	3.681382	0.001769	0.712715
-8.788734	-1.907687	3.691379	0.001831	0.712714
-8.731105	-1.917467	3.701376	0.001821	0.712715
-8.745862	-1.895673	3.711373	0.001824	0.712753
-7.614964	-1.957976	3.721370	0.001613	0.713029
-7.389237	-1.998211	3.731366	0.001571	0.713029
-7.676588	-1.949677	3.741363	0.001625	0.713023
-7.507705	-1.976764	3.751360	0.001594	0.713029
-6.656383	-1.960294	3.761357	0.001436	0.713363
-6.791442	-1.935866	3.771354	0.001461	0.713364
-6.467149	-1.993227	3.781350	0.001401	0.713364
-6.860417	-1.904618	3.791347	0.001474	0.713401
-6.103082	-1.907936	3.801344	0.001333	0.713662
-6.138575	-1.900027	3.811341	0.001340	0.713665
-5.953239	-1.935620	3.821338	0.001306	0.713660
-5.365133	-1.918215	3.831334	0.001196	0.713902
-4.963305	-1.953061	3.841331	0.001122	0.713975
-4.775913	-1.987881	3.851328	0.001087	0.713972
-5.045844	-1.932943	3.861325	0.001137	0.713985
-4.282628	-1.918194	3.871322	0.000995	0.714284
-4.086952	-1.955709	3.881318	0.000959	0.714278
-4.188955	-1.937643	3.891315	0.000978	0.714278
-3.793143	-1.922026	3.901312	0.000905	0.714449
-3.048822	-1.974602	3.911309	0.000766	0.714607
-3.094616	-1.963795	3.921306	0.000775	0.714612
-2.976981	-1.985127	3.931302	0.000753	0.714611
-2.531307	-1.964925	3.941299	0.000671	0.714808
-2.342822	-1.948569	3.951296	0.000636	0.714907
-2.235501	-1.967946	3.961293	0.000616	0.714906
-2.183102	-1.968643	3.971290	0.000606	0.714923
-1.513353	-1.929940	3.981286	0.000482	0.715236
-1.429027	-1.947190	3.991283	0.000466	0.715232
-1.426598	-1.948042	4.001280	0.000466	0.715230
-1.442477	-1.854522	4.011277	0.000469	0.715410
-1.177825	-1.833444	4.021274	0.000420	0.715545
-1.035388	-1.857774	4.031270	0.000394	0.715547
-1.057502	-1.729915	4.041267	0.000398	0.715792
-1.037037	-1.686558	4.051264	0.000394	0.715885
-0.900072	-1.675653	4.061261	0.000369	0.715955
-0.949091	-1.574245	4.071258	0.000378	0.716138
-0.694770	-1.591210	4.081254	0.000331	0.716194
-0.584325	-1.478285	4.091251	0.000311	0.716456
-0.590915	-1.451609	4.101248	0.000312	0.716506
-0.744774	-1.295700	4.111245	0.000341	0.716760
-0.719222	-1.223932	4.121242	0.000336	0.716911
-0.548684	-1.163199	4.131238	0.000304	0.717091
-0.335303	-1.077011	4.141235	0.000265	0.717336
-0.463906	-0.986025	4.151232	0.000289	0.717471
-0.455389	-0.868860	4.161229	0.000287	0.717705
-0.344877	-0.753372	4.171226	0.000267	0.717972
-0.243042	-0.666030	4.181222	0.000248	0.718180
-0.312397	-0.537531	4.191219	0.000261	0.718409
-0.180289	-0.442178	4.201216	0.000237	0.718644
-0.328799	-0.264750	4.211213	0.000264	0.718942
-0.223400	-0.150256	4.221210	0.000245	0.719204
0.056956	-0.065359	4.231206	0.000193	0.719470
-0.094321	0.102270	4.241203	0.000221	0.719747
0.000000	0.250318	4.251200	0.000203	0.720072

-0.015313	0.885265	4.256205	0.000206	0.721316
0.200692	2.101946	4.261210	0.000165	0.723781
0.510890	3.897067	4.266214	0.000106	0.727400
0.845797	6.248634	4.271219	0.000042	0.732089
0.734771	9.181824	4.276224	0.000061	0.737714
1.360795	12.456431	4.281229	-0.000057	0.744199
1.721985	16.239651	4.286234	-0.000127	0.751499
2.251812	20.398619	4.291238	-0.000228	0.759488
2.567290	24.996716	4.296243	-0.000290	0.768134
2.915826	29.956966	4.301248	-0.000358	0.777356
3.420843	35.233075	4.306253	-0.000455	0.787090
3.891743	40.840528	4.311258	-0.000547	0.797283
4.193030	46.765793	4.316262	-0.000606	0.807853
4.678670	52.961727	4.321267	-0.000701	0.818813
5.303033	59.385957	4.326272	-0.000821	0.830059
5.746277	66.086589	4.331277	-0.000908	0.841567
6.095568	73.015819	4.336282	-0.000977	0.853272
6.478943	80.138950	4.341286	-0.001053	0.865147
8.017654	87.260559	4.346291	-0.001344	0.877187
10.696745	94.377365	4.351296	-0.001848	0.889374
11.517399	102.007893	4.356301	-0.002006	0.901691
12.033752	109.835989	4.361306	-0.002107	0.914065
12.755416	117.737639	4.366310	-0.002246	0.926441
13.933168	125.692242	4.371315	-0.002471	0.938854
15.357296	133.714093	4.376320	-0.002741	0.951269
16.314475	141.910725	4.381325	-0.002924	0.963661
17.643453	150.136041	4.386330	-0.003177	0.976030
18.517218	158.527890	4.391334	-0.003345	0.988369
19.113757	167.016807	4.396339	-0.003462	1.000624
20.064043	175.465158	4.401344	-0.003644	1.012761
20.937635	183.988770	4.406349	-0.003812	1.024838
21.626138	192.579269	4.411354	-0.003946	1.036822
22.413028	201.177487	4.416358	-0.004098	1.048702
23.269306	209.791959	4.421363	-0.004263	1.060487
23.889695	218.457710	4.426368	-0.004384	1.072155
24.609093	227.101212	4.431373	-0.004523	1.083691
25.476764	235.728704	4.436378	-0.004690	1.095117
26.205272	244.376236	4.441382	-0.004832	1.106419
26.999295	253.031192	4.446387	-0.004985	1.117631
27.460995	261.729465	4.451392	-0.005077	1.128713
28.370097	270.356525	4.456397	-0.005251	1.139695
29.290251	278.997088	4.461402	-0.005428	1.150589
30.069487	287.633855	4.466406	-0.005579	1.161348
31.147326	296.211096	4.471411	-0.005785	1.171996
31.422397	304.894226	4.476416	-0.005842	1.182511
32.162029	313.508968	4.481421	-0.005985	1.192946
33.060363	322.064281	4.486426	-0.006158	1.203252
33.683073	330.666502	4.491430	-0.006279	1.213470
34.503163	339.234580	4.496435	-0.006438	1.223602
34.794142	347.887728	4.501440	-0.006497	1.233645
35.537677	356.420605	4.506445	-0.006641	1.243556
36.139134	364.967487	4.511450	-0.006759	1.253378
36.731481	373.489154	4.516454	-0.006874	1.263093
37.534345	381.987430	4.521459	-0.007029	1.272747
37.823822	390.523251	4.526464	-0.007089	1.282273
38.510243	399.006888	4.531469	-0.007222	1.291746
39.169814	407.464997	4.536474	-0.007350	1.301116
39.658299	416.005017	4.541478	-0.007447	1.310477
40.143561	424.541478	4.546483	-0.007542	1.319766
40.576178	432.963602	4.551488	-0.007628	1.328859
40.950937	441.407801	4.556493	-0.007704	1.337904
41.824478	449.731894	4.561498	-0.007872	1.346848
42.656871	458.098907	4.566502	-0.008032	1.355771
43.381557	466.461183	4.571507	-0.008172	1.364612
43.769708	474.873026	4.576512	-0.008250	1.373388
44.078096	483.290382	4.581517	-0.008313	1.382101
44.829980	491.625203	4.586522	-0.008458	1.390750
45.183148	500.018014	4.591526	-0.008529	1.399337
45.635528	508.376811	4.596531	-0.008619	1.407854
46.115036	516.718543	4.601536	-0.008713	1.416307
46.676028	525.036872	4.606541	-0.008823	1.424700
47.230478	533.382857	4.611546	-0.008932	1.433069
47.781460	541.672871	4.616550	-0.009040	1.441334
48.354503	549.992044	4.621555	-0.009152	1.449584
48.641037	558.342329	4.626560	-0.009210	1.457771
49.019401	566.656835	4.631565	-0.009286	1.465893
49.695953	574.971613	4.636570	-0.009418	1.474016
50.484749	583.197176	4.641574	-0.009570	1.482028
51.098516	591.463654	4.646579	-0.009689	1.490007
51.519340	599.749076	4.651584	-0.009773	1.497932
52.166725	607.983998	4.656589	-0.009899	1.505802
52.567075	616.292965	4.661594	-0.009979	1.513663
53.001149	624.539166	4.666598	-0.010065	1.521430
53.618838	632.791888	4.671603	-0.010185	1.529190
53.895433	641.087187	4.676608	-0.010242	1.536900
54.402701	649.326941	4.681613	-0.010342	1.544554
55.120076	657.559543	4.686618	-0.010480	1.552195
55.715273	665.780544	4.691622	-0.010597	1.559769
56.353079	673.996732	4.696627	-0.010721	1.567309
56.801728	682.245293	4.701632	-0.010809	1.574814
57.451016	690.449017	4.706637	-0.010936	1.582272
57.774744	698.709782	4.711642	-0.011001	1.589699
58.308079	706.929320	4.716646	-0.011106	1.597084
59.128137	715.098805	4.721651	-0.011264	1.604432
59.154643	723.396601	4.726656	-0.011274	1.611747
59.951064	731.569554	4.731661	-0.011427	1.619028
60.434164	739.784281	4.736666	-0.011523	1.626268
61.077169	748.024366	4.741670	-0.011648	1.633520
61.502965	756.237594	4.746675	-0.011732	1.640687
61.939677	764.430872	4.751680	-0.011819	1.647807
62.283780	772.660075	4.756685	-0.011888	1.654914
62.717622	780.838863	4.761690	-0.011974	1.661960
63.036573	789.038736	4.766694	-0.012039	1.668979
63.600059	797.232932	4.771699	-0.012149	1.675996
63.866910	805.420970	4.776704	-0.012204	1.682938
64.411022	813.577738	4.781709	-0.012310	1.689863
64.954333	821.749264	4.786714	-0.012417	1.696771
65.474603	829.899020	4.791718	-0.012519	1.703630
65.765836	838.125987	4.796723	-0.012578	1.710496
65.861203	846.350348	4.801728	-0.012601	1.717306
66.267961	854.502562	4.806733	-0.012682	1.724070
66.668710	862.673314	4.811738	-0.012762	1.730822
67.049302	870.840327	4.816742	-0.012838	1.737543
67.554923	879.008102	4.821747	-0.012938	1.744253
68.096945	887.139101	4.826752	-0.013044	1.750913
68.327289	895.339997	4.831757	-0.013092	1.757564
68.834782	903.463332	4.836762	-0.013192	1.764162
69.467601	911.569821	4.841766	-0.013315	1.770738
70.242985	919.700614	4.846771	-0.013464	1.777327
70.500262	927.886370	4.851776	-0.013517	1.783870
71.056798	936.058447	4.856781	-0.013626	1.790416
71.515370	944.255180	4.861786	-0.013717	1.796945
71.504509	952.429174	4.866790	-0.013720	1.803375
71.911929	960.581141	4.871795	-0.013801	1.809815
72.441799	968.695845	4.876800	-0.013905	1.816219
72.873936	976.838705	4.881805	-0.013991	1.822610
73.462876	984.961268	4.886810	-0.014106	1.828981
74.230956	993.064184	4.891814	-0.014254	1.835336
74.860576	1001.177190	4.896819	-0.014376	1.841661
75.023405	1009.350705	4.901824	-0.014412	1.847955
75.400219	1017.515643	4.906829	-0.014487	1.854246
75.814592	1025.649631	4.911834	-0.014570	1.860497
76.066909	1033.788997	4.916838	-0.014622	1.866711
76.400976	1041.973840	4.921843	-0.014689	1.872949
77.003354	1050.059504	4.926848	-0.014807	1.879122
77.380804	1058.168077	4.931853	-0.014882	1.885267
77.843662	1066.298841	4.936858	-0.014973	1.891417
78.108300	1074.456658	4.941862	-0.015028	1.897545
78.591677	1082.557417	4.946867	-0.015123	1.903636
78.765693	1090.721673	4.951872	-0.015161	1.909719
79.014115	1098.873663	4.956877	-0.015212	1.915783
79.673796	1106.932709	4.961882	-0.015340	1.921804
80.362358	1115.013069	4.966886	-0.015474	1.927825
80.922387	1123.149095	4.971891	-0.015583	1.933854
81.403069	1131.258364	4.976896	-0.015678	1.939835
81.537575	1139.413935	4.981901	-0.015708	1.945794
81.914859	1147.581079	4.986906	-0.015784	1.951770
82.411930	1155.676690	4.991910	-0.015881	1.957688
83.020836	1163.747847	4.996915	-0.016000	1.963583
83.118701	1171.887277	5.001920	-0.016023	1.969454
83.530153	1179.996962	5.006925	-0.016105	1.975320
83.975048	1188.089453	5.011930	-0.016193	1.981160
84.451480	1196.177870	5.016934	-0.016287	1.986983
84.943573	1204.312935	5.021939	-0.016384	1.992823
85.311022	1212.415858	5.026944	-0.016457	1.998610
85.791832	1220.503715	5.031949	-0.016552	2.004382
85.984703	1228.649449	5.036954	-0.016593	2.010148
86.072297	1236.800289	5.041958	-0.016615	2.015890
86.524229	1244.888202	5.046963	-0.016704	2.021609
86.792295	1252.991165	5.051968	-0.016759	2.027304
87.066995	1261.144640	5.056973	-0.016816	2.033018
87.714912	1269.200410	5.061978	-0.016941	2.038687
87.943786	1277.278608	5.066982	-0.016989	2.044312
88.394726	1285.371376	5.071987	-0.017078	2.049955
88.701892	1293.478159	5.076992	-0.017141	2.055577
89.242765	1301.544404	5.081997	-0.017247	2.061179
89.343172	1309.694781	5.087002	-0.017271	2.066780
89.659288	1317.795044	5.092006	-0.017335	2.072352
90.389686	1325.836955	5.097011	-0.017476	2.077911
90.635036	1333.931020	5.102016	-0.017527	2.083443
90.707773	1342.069541	5.107021	-0.017545	2.088972
91.443775	1350.142397	5.112026	-0.017688	2.094508
91.830861	1358.211031	5.117030	-0.017765	2.099992
92.135533	1366.334341	5.122035	-0.017827	2.105491
92.443390	1374.464713	5.127040	-0.017889	2.110980
92.915985	1382.577133	5.132045	-0.017983	2.116459
93.441236	1390.617507	5.137050	-0.018085	2.121880
93.644368	1398.713412	5.142054	-0.018129	2.127294
94.114752	1406.806349	5.147059	-0.018221	2.132717
94.289488	1414.910748	5.152064	-0.018259	2.138106
94.561547	1422.971233	5.157069	-0.018315	2.143461
95.006732	1431.063145	5.162074	-0.018403	2.148840
95.457490	1439.144006	5.167078	-0.018492	2.154199
95.941342	1447.219911	5.172083	-0.018587	2.159544
96.107710	1455.304553	5.177088	-0.018623	2.164852
96.509685	1463.395327	5.182093	-0.018703	2.170173
97.059727	1471.469189	5.187098	-0.018811	2.175483
97.454780	1479.548607	5.192102	-0.018890	2.180770
97.791831	1487.657591	5.197107	-0.018958	2.186058
98.032400	1495.774005	5.202112	-0.019008	2.191328
98.504621	1503.847427	5.207117	-0.019101	2.196580
99.000369	1511.894478	5.212122	-0.019198	2.201804
99.247211	1519.981432	5.217126	-0.019249	2.207018
99.546927	1528.094917	5.222131	-0.019310	2.212242
99.830174	1536.171672	5.227136	-0.019368	2.217429
100.276471	1544.219218	5.232141	-0.019457	2.222599
100.641068	1552.304150	5.237146	-0.019530	2.227774
100.823097	1560.416916	5.242150	-0.019569	2.232938
101.503455	1568.444280	5.247155	-0.019701	2.238080
101.873816	1576.510536	5.252160	-0.019775	2.243207
102.108952	1584.579123	5.257165	-0.019824	2.248312
102.694668	1592.664755	5.262170	-0.019938	2.253447
103.033757	1600.745178	5.267174	-0.020006	2.258546
103.525659	1608.809713	5.272179	-0.020103	2.263636
103.756470	1616.908856	5.277184	-0.020151	2.268714
104.285238	1625.061665	5.282189	-0.020255	2.273839
104.617977	1633.128320	5.287194	-0.020322	2.278882
104.773883	1641.172697	5.292198	-0.020356	2.283885
105.135983	1649.246876	5.297203	-0.020429	2.288913
105.465533	1657.326338	5.302208	-0.020495	2.293931
105.801065	1665.373460	5.307213	-0.020563	2.298918
106.078991	1673.449239	5.312218	-0.020620	2.303907
106.464208	1681.492653	5.317222	-0.020697	2.308874
106.802930	1689.597538	5.322227	-0.020765	2.313864
107.181430	1697.640048	5.327232	-0.020841	2.318809
107.592316	1705.669953	5.332237	-0.020922	2.323738
107.894275	1713.765662	5.337242	-0.020984	2.328688
108.040443	1721.865723	5.342246	-0.021016	2.333616
108.496639	1729.925516	5.347251	-0.021106	2.338536
108.799416	1737.993380	5.352256	-0.021168	2.343437
108.890797	1746.095264	5.357261	-0.021190	2.348331
109.218739	1754.190766	5.362266	-0.021256	2.353230
109.502449	1762.244035	5.367270	-0.021314	2.358091
110.008755	1770.270352	5.372275	-0.021414	2.362942
110.426940	1778.318304	5.377280	-0.021497	2.367790
110.823628	1786.379381	5.382285	-0.021576	2.372634
111.016399	1794.486364	5.387290	-0.021617	2.377479
111.136514	1802.548778	5.392294	-0.021644	2.382282
111.762877	1810.592851	5.397299	-0.021766	2.387104
111.937553	1818.684306	5.402304	-0.021804	2.391909
112.427610	1826.731117	5.407309	-0.021900	2.396702
112.899005	1834.774864	5.412314	-0.021993	2.401483
113.270155	1842.816147	5.417318	-0.022067	2.406244
113.568105	1850.906196	5.422323	-0.022128	2.411019
113.826778	1858.994502	5.427328	-0.022181	2.415781
114.207410	1867.039558	5.432333	-0.022257	2.420517
114.745250	1875.079881	5.437338	-0.022363	2.425253
114.900674	1883.181322	5.442342	-0.022397	2.429987
115.239308	1891.333932	5.447347	-0.022465	2.434754
115.603142	1899.341438	5.452352	-0.022538	2.439430
115.935104	1907.364150	5.457357	-0.022605	2.444103
116.154469	1915.438538	5.462362	-0.022651	2.448789
116.579168	1923.479756	5.467366	-0.022735	2.453462
117.093175	1931.517601	5.472371	-0.022836	2.458131
117.112174	1939.601653	5.477376	-0.022845	2.462780
117.445450	1947.647828	5.482381	-0.022912	2.467422
118.020932	1955.705985	5.487386	-0.023024	2.472081
117.994074	1963.813642	5.492390	-0.023024	2.476714
118.387737	1971.857594	5.497395	-0.023103	2.481333
118.776450	1979.875190	5.502400	-0.023180	2.485928
119.176023	1987.922689	5.507405	-0.023260	2.490532
119.666420	1995.997580	5.512410	-0.023356	2.495150
120.088074	2004.016056	5.517414	-0.023440	2.499723
120.437513	2012.090562	5.522419	-0.023510	2.504313
120.590395	2020.184869	5.527424	-0.023544	2.508892
120.932352	2028.278975	5.532429	-0.023613	2.513476
121.207736	2036.347421	5.537434	-0.023669	2.518032
121.482400	2044.352248	5.542438	-0.023726	2.522544
121.652000	2052.441894	5.547443	-0.023762	2.527088
121.959633	2060.480846	5.552448	-0.023825	2.531606
122.392438	2068.520669	5.557453	-0.023910	2.536124
122.516877	2076.605316	5.562458	-0.023939	2.540638
122.864860	2084.620452	5.567462	-0.024009	2.545121
122.959922	2092.733473	5.572467	-0.024032	2.549632
123.323548	2100.785247	5.577472	-0.024104	2.554120
123.682075	2108.808293	5.582477	-0.024176	2.558584
123.989403	2116.874382	5.587482	-0.024239	2.563060
124.146562	2124.925782	5.592486	-0.024273	2.567510
124.500382	2132.979882	5.597491	-0.024344	2.571968
124.767363	2141.046279	5.602496	-0.024399	2.576418
125.040553	2149.086709	5.607501	-0.024455	2.580847
125.296183	2157.140468	5.612506	-0.024508	2.585274
125.364966	2165.194373	5.617510	-0.024526	2.589681
125.677015	2173.449896	5.622515	-0.024589	2.594206
125.977322	2181.430084	5.627520	-0.024650	2.598574
126.101016	2189.442966	5.632525	-0.024678	2.602939
126.374304	2197.455423	5.637530	-0.024734	2.607307
126.731264	2205.476889	5.642534	-0.024806	2.611679
126.877257	2213.551974	5.647539	-0.024838	2.616057
127.335022	2221.545488	5.652544	-0.024929	2.620406
127.693325	2229.553818	5.657549	-0.025001	2.624748
128.136721	2237.602881	5.662554	-0.025088	2.629110
128.256287	2245.683592	5.667558	-0.025116	2.633461
128.505832	2253.746945	5.672563	-0.025167	2.637804
128.862829	2261.765374	5.677568	-0.025239	2.642123
129.008402	2269.822129	5.682573	-0.025271	2.646441
129.497749	2277.852786	5.687578	-0.025368	2.650761
129.776849	2285.926288	5.692582	-0.025425	2.655082
130.133441	2293.978145	5.697587	-0.025496	2.659390
130.503558	2301.998116	5.702592	-0.025570	2.663675
130.784659	2310.057343	5.707597	-0.025628	2.667968
130.953673	2318.157465	5.712602	-0.025664	2.672269
131.098413	2326.216358	5.717606	-0.025697	2.676539
131.503446	2334.223047	5.722611	-0.025777	2.680792
131.731223	2342.244501	5.727616	-0.025825	2.685034
131.937527	2350.303929	5.732621	-0.025868	2.689288
132.374164	2358.356896	5.737626	-0.025955	2.693546
132.595514	2366.387941	5.742630	-0.026001	2.697773
132.826925	2374.437672	5.747635	-0.026049	2.702003
133.064608	2382.495228	5.752640	-0.026099	2.706231
133.393227	2390.530140	5.757645	-0.026165	2.710447
133.836584	2398.601847	5.762650	-0.026253	2.714682
134.104724	2406.614220	5.767654	-0.026308	2.718868
134.434023	2414.660701	5.772659	-0.026374	2.723070
134.682197	2422.711362	5.777664	-0.026426	2.727262
134.883292	2430.777119	5.782669	-0.026468	2.731453
135.331893	2438.840029	5.787674	-0.026557	2.735650
135.495247	2446.857894	5.792678	-0.026593	2.739801
135.856707	2454.899826	5.797683	-0.026665	2.743970
136.160953	2462.959717	5.802688	-0.026727	2.748138
136.323138	2471.060861	5.807693	-0.026762	2.752313
136.724581	2479.150016	5.812698	-0.026842	2.756489
136.958298	2487.135969	5.817702	-0.026891	2.760596
137.300586	2495.142641	5.822707	-0.026960	2.764714
137.439557	2503.180881	5.827712	-0.026991	2.768830
137.547876	2511.245146	5.832717	-0.027016	2.772951
138.007333	2519.275149	5.837722	-0.027107	2.777069
138.160096	2527.302562	5.842726	-0.027140	2.781161
138.287552	2535.359586	5.847731	-0.027169	2.785262
138.557615	2543.406528	5.852736	-0.027225	2.789359
138.861615	2551.454143	5.857741	-0.027286	2.793452
139.262557	2559.492068	5.862746	-0.027366	2.797541
139.514962	2567.501533	5.867750	-0.027418	2.801600
139.982427	2575.522849	5.872755	-0.027510	2.805672
140.436358	2583.560121	5.877760	-0.027600	2.809745
140.541501	2591.656071	5.882765	-0.027625	2.813821
140.959633	2599.696331	5.887770	-0.027708	2.817881
141.280178	2607.714065	5.892774	-0.027773	2.821919
141.446137	2615.784785	5.897779	-0.027809	2.825969
141.743857	2623.830331	5.902784	-0.027869	2.830007
142.056095	2631.900917	5.907789	-0.027933	2.834053
142.307362	2639.932459	5.912794	-0.027985	2.838071
142.655079	2647.933865	5.917798	-0.028054	2.842073
143.267663	2655.949541	5.922803	-0.028174	2.846091
143.426461	2664.004100	5.927808	-0.028208	2.850098
143.617051	2672.065882	5.932813	-0.028249	2.854104
144.271445	2680.078824	5.937818	-0.028376	2.858106
144.467374	2688.097224	5.942822	-0.028418	2.862080
144.831844	2696.162467	5.947827	-0.028491	2.866080
145.108030	2704.200235	5.952832	-0.028547	2.870057
145.217668	2712.284382	5.957837	-0.028573	2.874041
145.622259	2720.324107	5.962842	-0.028653	2.878015
145.628267	2728.352612	5.967846	-0.028660	2.881955
146.184540	2736.360415	5.972851	-0.028768	2.885910
146.449328	2744.413697	5.977856	-0.028823	2.889866
146.396689	2752.491509	5.982861	-0.028818	2.893811
146.820748	2760.534143	5.987866	-0.028902	2.897760
147.081775	2768.554019	5.992870	-0.028956	2.901683
147.464388	2776.592713	5.997875	-0.029032	2.905616
147.418943	2784.666344	6.002880	-0.029029	2.909539
147.869811	2792.755060	6.007885	-0.029118	2.913489
148.154531	2800.806150	6.012890	-0.029176	2.917407
148.193184	2808.811833	6.017894	-0.029189	2.921285
148.545968	2816.791380	6.022899	-0.029260	2.925162
148.868262	2824.825785	6.027904	-0.029325	2.929058
148.975626	2832.885974	6.032909	-0.029350	2.932950
149.394876	2840.940014	6.037914	-0.029433	2.936850
149.638321	2848.908374	6.042918	-0.029483	2.940695
149.994735	2856.921287	6.047923	-0.029555	2.944562
150.076371	2865.011665	6.052928	-0.029575	2.948447
150.273720	2873.047491	6.057933	-0.029617	2.952306
150.771764	2881.108684	6.062938	-0.029715	2.956188
150.828912	2889.107020	6.067942	-0.029731	2.960012
151.079347	2897.144168	6.072947	-0.029783	2.963860
151.551030	2905.165657	6.077952	-0.029876	2.967706
151.883575	2913.216577	6.082957	-0.029943	2.971554
151.931180	2921.299224	6.087962	-0.029957	2.975398
152.184634	2929.293495	6.092966	-0.030009	2.979205
152.577887	2937.320223	6.097971	-0.030087	2.983030
152.777993	2945.369320	6.102976	-0.030130	2.986851
153.170578	2953.403229	6.107981	-0.030208	2.990669
153.402496	2961.498954	6.112986	-0.030256	2.994503
153.739345	2969.491474	6.117990	-0.030324	2.998290
153.942808	2977.528182	6.122995	-0.030367	3.002085
154.237708	2985.545006	6.128000	-0.030427	3.005871
154.384507	2993.576951	6.133005	-0.030460	3.009651
154.638762	3001.683094	6.138010	-0.030512	3.013467
154.757212	3009.697146	6.143014	-0.030540	3.017229
155.065748	3017.717516	6.148019	-0.030602	3.020998
155.259120	3025.733294	6.153024	-0.030643	3.024754
155.385350	3033.770116	6.158029	-0.030672	3.028512
155.759507	3041.822172	6.163034	-0.030747	3.032285
155.937766	3049.870469	6.168038	-0.030785	3.036042
156.112582	3057.880832	6.173043	-0.030823	3.039776
156.318757	3065.917420	6.178048	-0.030866	3.043519
156.399801	3073.948580	6.183053	-0.030887	3.047249
156.721741	3081.997985	6.188058	-0.030952	3.050995
156.958810	3090.040486	6.193062	-0.031001	3.054728
157.599217	3098.026119	6.198067	-0.031125	3.058450
157.896439	3106.071655	6.203072	-0.031186	3.062179
158.088163	3114.112817	6.208077	-0.031227	3.065896
158.433156	3122.155077	6.213082	-0.031296	3.069616
158.621360	3130.284951	6.218086	-0.031336	3.073365
158.858090	3138.304367	6.223091	-0.031386	3.077060
159.085092	3146.311387	6.228096	-0.031433	3.080745
159.122912	3154.311721	6.233101	-0.031445	3.084414
159.505235	3162.343631	6.238106	-0.031521	3.088108
159.625376	3170.391157	6.243110	-0.031549	3.091794
159.697920	3178.433280	6.248115	-0.031568	3.095470
159.867970	3186.454040	6.253120	-0.031604	3.099136
160.220141	3194.455267	6.258125	-0.031675	3.102798
160.554981	3202.505612	6.263130	-0.031743	3.106476
160.778904	3210.531330	6.268134	-0.031789	3.110134
161.063540	3218.595007	6.273139	-0.031848	3.113808
161.408882	3226.616199	6.278144	-0.031917	3.117461
161.646544	3234.642437	6.283149	-0.031966	3.121107
162.044390	3242.636860	6.288154	-0.032046	3.124741
162.242667	3250.677009	6.293158	-0.032088	3.128383
162.591858	3258.717366	6.298163	-0.032158	3.132027
162.863012	3266.770755	6.303168	-0.032214	3.135670
163.098290	3274.774721	6.308173	-0.032262	3.139284
163.420550	3282.833730	6.313178	-0.032328	3.142923
163.692332	3290.845970	6.318182	-0.032383	3.146534
163.914224	3298.879364	6.323187	-0.032430	3.150148
164.061595	3306.972540	6.328192	-0.032462	3.153782
164.075829	3315.001485	6.333197	-0.032470	3.157377
164.561337	3323.002484	6.338202	-0.032566	3.160976
164.574478	3331.014298	6.343206	-0.032573	3.164555
164.899302	3339.022034	6.348211	-0.032639	3.168141
165.075489	3347.100941	6.353216	-0.032677	3.171749
165.190874	3355.126190	6.358221	-0.032704	3.175326
165.530052	3363.164463	6.363226	-0.032772	3.178915
165.824816	3371.156445	6.368230	-0.032832	3.182476
166.285414	3379.186116	6.373235	-0.032923	3.186058
166.469783	3387.247766	6.378240	-0.032962	3.189638
166.567386	3395.282333	6.383245	-0.032986	3.193198
166.668369	3403.372940	6.388250	-0.033010	3.196780
166.869375	3411.344408	6.393254	-0.033052	3.200308
167.126092	3419.345734	6.398259	-0.033105	3.203849
167.465928	3427.390767	6.403264	-0.033174	3.207408
167.766547	3435.423751	6.408269	-0.033235	3.210956
167.933517	3443.482547	6.413274	-0.033271	3.214506
168.083432	3451.496455	6.418278	-0.033304	3.218032
168.403636	3459.525438	6.423283	-0.033369	3.221567
168.642661	3467.540303	6.428288	-0.033418	3.225089
168.946334	3475.576609	6.433293	-0.033480	3.228619
169.402370	3483.659912	6.438298	-0.033570	3.232172
169.720404	3491.683561	6.443302	-0.033634	3.235689
170.023718	3499.676651	6.448307	-0.033696	3.239189
170.246112	3507.690286	6.453312	-0.033743	3.242690
170.404982	3515.712791	6.458317	-0.033777	3.246189
170.562799	3523.748443	6.463322	-0.033812	3.249689
170.814117	3531.776386	6.468326	-0.033864	3.253187
170.955662	3539.854066	6.473331	-0.033895	3.256697
171.044186	3547.877625	6.478336	-0.033917	3.260179
171.512214	3555.858027	6.483341	-0.034009	3.263653
171.708837	3563.921596	6.488346	-0.034051	3.267148
171.889475	3571.959924	6.493350	-0.034090	3.270628
172.144670	3580.014657	6.498355	-0.034142	3.274114
172.512427	3588.023775	6.503360	-0.034216	3.277582
172.661805	3596.045225	6.508365	-0.034249	3.281042
172.963389	3604.086990	6.513370	-0.034310	3.284514
173.275261	3612.086346	6.518374	-0.034374	3.287963
173.630300	3620.128971	6.523379	-0.034445	3.291430
173.728166	3628.182035	6.528384	-0.034468	3.294887
173.796431	3636.196661	6.533389	-0.034486	3.298323
174.145003	3644.200670	6.538394	-0.034556	3.301762
174.113981	3652.202942	6.543398	-0.034555	3.305181
174.583072	3660.238832	6.548403	-0.034648	3.308631
174.826813	3668.313441	6.553408	-0.034698	3.312085
175.061358	3676.335845	6.558413	-0.034747	3.315513
175.320605	3684.374042	6.563418	-0.034801	3.318944
175.538018	3692.381017	6.568422	-0.034846	3.322358
175.677121	3700.403909	6.573427	-0.034877	3.325771
175.818532	3708.429764	6.578432	-0.034909	3.329183
175.991149	3716.454584	6.583437	-0.034946	3.332591
176.311029	3724.516244	6.588442	-0.035011	3.336017
176.379300	3732.518047	6.593446	-0.035029	3.339405
176.483220	3740.540459	6.598451	-0.035053	3.342800
176.745544	3748.567798	6.603456	-0.035107	3.346199
176.974206	3756.587071	6.608461	-0.035155	3.349589
177.372407	3764.655650	6.613466	-0.035234	3.353004
177.728834	3772.679829	6.618470	-0.035306	3.356394
177.962300	3780.673766	6.623475	-0.035354	3.359764
178.226682	3788.715597	6.628480	-0.035409	3.363152
178.452525	3796.731729	6.633485	-0.035456	3.366524
178.566773	3804.786329	6.638490	-0.035482	3.369905
178.711556	3812.836804	6.643494	-0.035514	3.373281
179.032609	3820.873835	6.648499	-0.035579	3.376655
179.396763	3828.864621	6.653504	-0.035652	3.380008
179.476894	3836.861182	6.658509	-0.035672	3.383350
179.809699	3844.920161	6.663514	-0.035739	3.386723
180.025078	3852.931941	6.668518	-0.035785	3.390069
180.757490	3860.993434	6.673523	-0.035926	3.393451
181.264709	3869.060271	6.678528	-0.036026	3.396823
181.373283	3877.021841	6.683533	-0.036051	3.400135
181.824518	3885.028342	6.688538	-0.036140	3.403473
181.951492	3893.050867	6.693542	-0.036169	3.406804
182.184822	3901.061239	6.698547	-0.036218	3.410130
182.546683	3909.119557	6.703552	-0.036290	3.413478
182.702490	3917.149213	6.708557	-0.036324	3.416802
182.893911	3925.190664	6.713562	-0.036365	3.420130
183.072010	3933.183600	6.718566	-0.036403	3.423434
183.313344	3941.208753	6.723571	-0.036453	3.426750
183.509197	3949.245493	6.728576	-0.036495	3.430067
183.568629	3957.287494	6.733581	-0.036511	3.433377
183.953199	3965.336099	6.738586	-0.036588	3.436698
184.023276	3973.353368	6.743590	-0.036606	3.439992
184.364039	3981.350506	6.748595	-0.036675	3.443284
184.640818	3989.379649	6.753600	-0.036731	3.446584
184.616164	3997.422433	6.758605	-0.036732	3.449876
184.742093	4005.496766	6.763610	-0.036761	3.453183
185.176788	4013.520689	6.768614	-0.036847	3.456476
185.295003	4021.485802	6.773619	-0.036874	3.459732
185.669278	4029.549234	6.778624	-0.036949	3.463032
185.729525	4037.567938	6.783629	-0.036965	3.466302
186.163798	4045.603894	6.788634	-0.037051	3.469587
186.320089	4053.648800	6.793638	-0.037085	3.472864
186.352606	4061.693411	6.798643	-0.037096	3.476134
186.618636	4069.687336	6.803648	-0.037151	3.479387
186.893196	4077.665874	6.808653	-0.037207	3.482631
187.131850	4085.685616	6.813658	-0.037257	3.485888
187.278909	4093.662218	6.818662	-0.037289	3.489122
187.486434	4101.743560	6.823667	-0.037333	3.492396
187.937569	4109.812224	6.828672	-0.037422	3.495671
188.022785	4117.796929	6.833677	-0.037443	3.498896
188.482737	4125.850088	6.838682	-0.037534	3.502158
188.519373	4133.837223	6.843686	-0.037546	3.505377
188.656074	4141.883819	6.848691	-0.037577	3.508620
188.963819	4149.954399	6.853696	-0.037639	3.511875
189.083578	4157.957516	6.858701	-0.037667	3.515094
189.463813	4165.964606	6.863706	-0.037743	3.518320
189.629501	4174.011822	6.868710	-0.037779	3.521552
189.862325	4181.975693	6.873715	-0.037827	3.524750
189.987247	4190.049450	6.878720	-0.037855	3.527986
190.082846	4198.076653	6.883725	-0.037878	3.531199
190.426178	4206.125495	6.888730	-0.037947	3.534425
190.677577	4214.145690	6.893734	-0.037999	3.537634
190.784995	4222.160525	6.898739	-0.038025	3.540834
191.132569	4230.176577	6.903744	-0.038094	3.544038
191.393447	4238.197846	6.908749	-0.038148	3.547239
191.699466	4246.245139	6.913754	-0.038210	3.550449
191.788130	4254.374836	6.918758	-0.038232	3.553682
191.991902	4262.368205	6.923763	-0.038275	3.556862
192.204877	4270.385475	6.928768	-0.038320	3.560048
192.402479	4278.322886	6.933773	-0.038362	3.563199
192.517273	4286.352343	6.938778	-0.038388	3.566382
192.843353	4294.319185	6.943782	-0.038454	3.569543
192.953264	4302.392692	6.948787	-0.038480	3.572737
193.393295	4310.422706	6.953792	-0.038567	3.575921
193.545077	4318.404881	6.958797	-0.038600	3.579074
193.744016	4326.469223	6.963802	-0.038642	3.582259
193.854593	4334.475803	6.968806	-0.038668	3.585415
193.929667	4342.506323	6.973811	-0.038687	3.588577
194.240605	4350.589106	6.978816	-0.038750	3.591763
194.470041	4358.566531	6.983821	-0.038798	3.594903
194.714026	4366.612885	6.988826	-0.038849	3.598068
195.039260	4374.570675	6.993830	-0.038914	3.601197
195.132224	4382.564689	6.998835	-0.038937	3.604331
195.376225	4390.654830	7.003840	-0.038987	3.607504
195.721271	4398.655667	7.008845	-0.039057	3.610642
195.768439	4406.732439	7.013850	-0.039071	3.613799
196.058897	4414.734515	7.018854	-0.039130	3.616931
196.331313	4422.730506	7.023859	-0.039186	3.620057
196.674061	4430.781556	7.028864	-0.039255	3.623204
196.634492	4438.815687	7.033869	-0.039253	3.626331
196.798906	4446.845074	7.038874	-0.039288	3.629459
197.128311	4454.902260	7.043878	-0.039355	3.632599
197.429878	4462.933900	7.048883	-0.039416	3.635726
197.475470	4470.925711	7.053888	-0.039430	3.638828
197.785345	4478.907951	7.058893	-0.039492	3.641931
197.996137	4486.935333	7.063898	-0.039537	3.645046
198.340043	4494.947742	7.068902	-0.039606	3.648155
198.374760	4503.011485	7.073907	-0.039618	3.651274
198.796383	4511.053630	7.078912	-0.039701	3.654392
198.841165	4519.086101	7.083917	-0.039715	3.657494
198.772913	4527.133806	7.088922	-0.039707	3.660596
199.004460	4535.103433	7.093926	-0.039755	3.663673
198.934820	4543.128335	7.098931	-0.039748	3.666761
199.195279	4551.153469	7.103936	-0.039801	3.669855
199.429176	4559.177507	7.108941	-0.039850	3.672945
199.539488	4567.226338	7.113946	-0.039876	3.676039
199.887511	4575.189024	7.118950	-0.039946	3.679103
200.169124	4583.206862	7.123955	-0.040003	3.682184
200.497577	4591.229297	7.128960	-0.040069	3.685266
200.604105	4599.236367	7.133965	-0.040094	3.688333
200.835752	4607.319600	7.138970	-0.040143	3.691430
201.101906	4615.338016	7.143974	-0.040197	3.694501
201.273860	4623.357868	7.148979	-0.040235	3.697567
201.565053	4631.366947	7.153984	-0.040294	3.700629
201.752833	4639.329625	7.158989	-0.040334	3.703669
202.007664	4647.420936	7.163994	-0.040387	3.706756
201.924650	4655.442206	7.168998	-0.040376	3.709806
202.065634	4663.533818	7.174003	-0.040408	3.712886
202.473507	4671.567586	7.179008	-0.040489	3.715948
202.626976	4679.509075	7.184013	-0.040522	3.718966
202.962402	4687.545251	7.189018	-0.040590	3.722022
203.131028	4695.527801	7.194022	-0.040627	3.725051
203.402805	4703.522834	7.199027	-0.040682	3.728085
203.481525	4711.596841	7.204032	-0.040702	3.731141
203.703604	4719.606609	7.209037	-0.040749	3.734174
204.193832	4727.610469	7.214042	-0.040845	3.737209
204.421327	4735.622434	7.219046	-0.040893	3.740238
204.589542	4743.639691	7.224051	-0.040929	3.743265
205.113494	4751.693852	7.229056	-0.041032	3.746311
205.063556	4759.673865	7.234061	-0.041028	3.749315
205.328027	4767.791319	7.239066	-0.041082	3.752374
205.664083	4775.789838	7.244070	-0.041150	3.755388
206.225708	4783.772918	7.249075	-0.041259	3.758399
206.452892	4791.858648	7.254080	-0.041307	3.761438
206.772923	4799.787150	7.259085	-0.041371	3.764418
207.096036	4807.849449	7.264090	-0.041437	3.767446
207.162324	4815.923771	7.269094	-0.041454	3.770470
207.478605	4823.947084	7.274099	-0.041518	3.773478
207.671427	4832.000178	7.279104	-0.041559	3.776492
207.790501	4839.944577	7.284109	-0.041587	3.779461
207.926842	4848.000562	7.289114	-0.041617	3.782470
208.122892	4855.995843	7.294118	-0.041659	3.785455
208.496375	4864.030693	7.299123	-0.041734	3.788457
208.753042	4872.117525	7.304128	-0.041787	3.791473
208.787509	4880.110531	7.309133	-0.041798	3.794446
208.981111	4888.135023	7.314138	-0.041839	3.797433
209.177980	4896.113591	7.319142	-0.041881	3.800400
209.420756	4904.108460	7.324147	-0.041931	3.803372
209.642420	4912.147131	7.329152	-0.041978	3.806357
209.733437	4920.117102	7.334157	-0.042000	3.809312
209.921704	4928.191516	7.339162	-0.042040	3.812305
210.236048	4936.206917	7.344166	-0.042104	3.815276
210.468276	4944.213941	7.349171	-0.042152	3.818241
210.668315	4952.267175	7.354176	-0.042194	3.821219
210.821868	4960.237159	7.359181	-0.042228	3.824164
211.216678	4968.271787	7.364186	-0.042307	3.827134
211.411658	4976.280805	7.369190	-0.042348	3.830089
211.791715	4984.334969	7.374195	-0.042424	3.833063
212.148207	4992.370552	7.379200	-0.042496	3.836026
212.140454	5000.356237	7.384205	-0.042499	3.838961
212.235142	5008.381492	7.389210	-0.042522	3.841911
212.575864	5016.375592	7.394214	-0.042591	3.844852
212.825523	5024.428653	7.399219	-0.042642	3.847810
212.908597	5032.474974	7.404224	-0.042663	3.850761
213.098879	5040.490112	7.409229	-0.042704	3.853699
213.341453	5048.531667	7.414234	-0.042754	3.856646
213.543718	5056.547495	7.419238	-0.042797	3.859581
213.642184	5064.556303	7.424243	-0.042820	3.862509
213.902352	5072.593359	7.429248	-0.042874	3.865448
214.096671	5080.615342	7.434253	-0.042915	3.868378
214.241660	5088.633275	7.439258	-0.042947	3.871303
214.292289	5096.907598	7.444262	-0.042962	3.874318
214.437475	5104.831544	7.449267	-0.042994	3.877205
214.756498	5112.748869	7.454272	-0.043058	3.880090
214.891229	5120.733473	7.459277	-0.043089	3.882994
215.194081	5128.779835	7.464282	-0.043150	3.885921
215.339739	5136.745048	7.469286	-0.043182	3.888814
215.491541	5144.732309	7.474291	-0.043216	3.891713
215.524787	5152.853278	7.479296	-0.043227	3.894656
215.834116	5160.819530	7.484301	-0.043290	3.897546
216.025746	5168.834997	7.489306	-0.043331	3.900449
216.013874	5176.863472	7.494310	-0.043334	3.903351
216.088229	5184.882293	7.499315	-0.043353	3.906249
216.427772	5192.887598	7.504320	-0.043421	3.909144
216.481883	5200.911683	7.509325	-0.043436	3.912039
216.808080	5208.934979	7.514330	-0.043502	3.914937
217.075482	5216.956041	7.519334	-0.043557	3.917830
217.227075	5224.947281	7.524339	-0.043590	3.920709
217.679464	5232.972060	7.529344	-0.043680	3.923602
217.953029	5240.998787	7.534349	-0.043736	3.926492
218.013963	5249.027258	7.539354	-0.043752	3.929375
218.156814	5257.079394	7.544358	-0.043784	3.932267
218.449552	5265.055274	7.549363	-0.043844	3.935132
218.538684	5273.118508	7.554368	-0.043865	3.938022
218.728562	5281.080751	7.559373	-0.043906	3.940876
218.984621	5289.124224	7.564378	-0.043959	3.943758
219.175108	5297.159382	7.569382	-0.043999	3.946634
219.229282	5305.158069	7.574387	-0.044015	3.949492
219.509877	5313.234881	7.579392	-0.044072	3.952380
219.681334	5321.235362	7.584397	-0.044109	3.955236
219.918700	5329.275386	7.589402	-0.044158	3.958106
220.062770	5337.286297	7.594406	-0.044190	3.960962
220.374772	5345.252170	7.599411	-0.044254	3.963802
220.349539	5353.287974	7.604416	-0.044254	3.966660
220.462624	5361.266883	7.609421	-0.044280	3.969497
220.769758	5369.343682	7.614426	-0.044342	3.972371
221.092667	5377.366776	7.619430	-0.044408	3.975223
221.315017	5385.340519	7.624435	-0.044454	3.978055
221.652696	5393.387909	7.629440	-0.044522	3.980912
221.683038	5401.376758	7.634445	-0.044533	3.983741
222.023936	5409.425160	7.639450	-0.044602	3.986595
222.317281	5417.444536	7.644454	-0.044661	3.989435
222.499317	5425.476539	7.649459	-0.044700	3.992276
222.624482	5433.544316	7.654464	-0.044729	3.995127
222.778840	5441.550229	7.659469	-0.044763	3.997954
223.044864	5449.538320	7.664474	-0.044817	4.000775
223.340915	5457.555657	7.669478	-0.044878	4.003604
223.128039	5465.564847	7.674483	-0.044843	4.006421
223.396736	5473.612620	7.679488	-0.044898	4.009257
223.624671	5481.644896	7.684493	-0.044946	4.012084
223.949081	5489.673416	7.689498	-0.045012	4.014910
224.187855	5497.715000	7.694502	-0.045061	4.017737
224.561322	5505.664869	7.699507	-0.045136	4.020532
224.977386	5513.705016	7.704512	-0.045218	4.023357
224.903826	5521.730882	7.709517	-0.045210	4.026168
225.020290	5529.739989	7.714522	-0.045237	4.028974
225.273429	5537.779309	7.719526	-0.045289	4.031790
225.403876	5545.887592	7.724531	-0.045318	4.034627
225.694311	5553.884990	7.729536	-0.045378	4.037425
225.977294	5561.825756	7.734541	-0.045435	4.040201
226.189938	5569.840376	7.739546	-0.045480	4.043000
226.475495	5577.824493	7.744550	-0.045538	4.045788
226.649488	5585.856477	7.749555	-0.045576	4.048589
227.064523	5593.898600	7.754560	-0.045658	4.051395
227.032692	5601.903624	7.759565	-0.045658	4.054179
227.424938	5609.944579	7.764570	-0.045736	4.056980
227.718175	5617.912553	7.769574	-0.045795	4.059752
227.747910	5625.932654	7.774579	-0.045806	4.062537
228.131104	5633.954972	7.779584	-0.045883	4.065326
228.300886	5641.962618	7.784589	-0.045919	4.068104
228.329360	5650.021063	7.789594	-0.045930	4.070897
228.649536	5658.061864	7.794598	-0.045995	4.073685
228.724010	5666.046618	7.799603	-0.046014	4.076449
228.974418	5674.035399	7.804608	-0.046065	4.079214
229.132360	5682.064932	7.809613	-0.046100	4.081990
229.320856	5690.062646	7.814618	-0.046140	4.084754
229.598869	5698.098636	7.819622	-0.046197	4.087531
229.697893	5706.105377	7.824627	-0.046221	4.090293
229.727377	5714.174600	7.829632	-0.046231	4.093074
229.873809	5722.176890	7.834637	-0.046264	4.095831
230.088695	5730.194777	7.839642	-0.046309	4.098593
230.348761	5738.231012	7.844646	-0.046362	4.101359
230.464198	5746.189099	7.849651	-0.046389	4.104095
230.653224	5754.259874	7.854656	-0.046429	4.106869
230.947802	5762.234024	7.859661	-0.046489	4.109610
231.138079	5770.336740	7.864666	-0.046530	4.112391
231.384299	5778.406541	7.869670	-0.046581	4.115159
231.484657	5786.354024	7.874675	-0.046605	4.117882
231.578153	5794.368202	7.879680	-0.046627	4.120626
231.833616	5802.357317	7.884685	-0.046680	4.123362
232.062438	5810.375642	7.889690	-0.046728	4.126105
232.333157	5818.437242	7.894694	-0.046783	4.128862
232.272795	5826.457444	7.899699	-0.046777	4.131598
232.778582	5834.439323	7.904704	-0.046876	4.134327
232.873711	5842.503289	7.909709	-0.046899	4.137077
233.019347	5850.508575	7.914714	-0.046932	4.139806
233.135163	5858.567944	7.919718	-0.046958	4.142550
233.302406	5866.537313	7.924723	-0.046995	4.145263
233.475022	5874.603662	7.929728	-0.047032	4.148008
233.586384	5882.588335	7.934733	-0.047058	4.150722
233.745272	5890.624522	7.939738	-0.047092	4.153452
233.857481	5898.681438	7.944742	-0.047118	4.156187
233.954731	5906.633682	7.949747	-0.047142	4.158884
234.220828	5914.683256	7.954752	-0.047196	4.161615
234.437787	5922.632862	7.959757	-0.047242	4.164309
234.686435	5930.675276	7.964762	-0.047293	4.167033
234.718867	5938.695910	7.969766	-0.047304	4.169746
234.869231	5946.727226	7.974771	-0.047338	4.172462
235.228556	5954.765467	7.979776	-0.047410	4.175180
235.222549	5962.772627	7.984781	-0.047414	4.177883
235.605314	5970.775443	7.989786	-0.047490	4.180586
235.795682	5978.785027	7.994790	-0.047531	4.183288
235.833123	5986.788895	7.999795	-0.047543	4.185984
236.202723	5994.840506	8.004800	-0.047617	4.188699
236.220890	6002.879573	8.009805	-0.047625	4.191403
236.438540	6011.013408	8.014810	-0.047671	4.194140
236.626089	6018.997406	8.019814	-0.047711	4.196824
236.920066	6026.881060	8.024819	-0.047771	4.199474
237.272142	6034.939330	8.029824	-0.047842	4.202182
237.130301	6042.878012	8.034829	-0.047820	4.204842
237.474253	6050.921872	8.039834	-0.047889	4.207541
237.711392	6058.936895	8.044838	-0.047939	4.210228
237.638017	6066.984906	8.049843	-0.047930	4.212920
237.786402	6075.027852	8.054848	-0.047963	4.215612
238.098935	6082.976892	8.059853	-0.048026	4.218272
238.267616	6091.007206	8.064858	-0.048063	4.220956
238.346187	6099.026567	8.069862	-0.048083	4.223634
238.515601	6107.019463	8.074867	-0.048119	4.226302
238.827586	6115.109961	8.079872	-0.048183	4.229002
238.817541	6123.110715	8.084877	-0.048186	4.231667
238.922912	6131.167717	8.089882	-0.048211	4.234351
239.118127	6139.176725	8.094886	-0.048252	4.237018
239.369783	6147.093533	8.099891	-0.048304	4.239653
239.646787	6155.163162	8.104896	-0.048361	4.242337
239.873146	6163.129372	8.109901	-0.048408	4.244985
240.067683	6171.205006	8.114906	-0.048449	4.247667
240.352206	6179.229776	8.119910	-0.048507	4.250331
240.434832	6187.250896	8.124915	-0.048528	4.252991
240.609551	6195.285038	8.129920	-0.048566	4.255654
240.609865	6203.282599	8.134925	-0.048571	4.258302
240.938148	6211.305010	8.139930	-0.048637	4.260959
241.197465	6219.345667	8.144934	-0.048691	4.263620
241.313953	6227.332710	8.149939	-0.048717	4.266260
241.267515	6235.416806	8.154944	-0.048714	4.268929
241.421791	6243.430912	8.159949	-0.048748	4.271576
241.755551	6251.438034	8.164954	-0.048815	4.274219
241.895360	6259.491030	8.169958	-0.048846	4.276875
241.976152	6267.399798	8.174963	-0.048866	4.279481
242.205932	6275.526105	8.179968	-0.048914	4.282158
242.444909	6283.412482	8.184973	-0.048964	4.284755
242.582552	6291.493267	8.189978	-0.048995	4.287413
243.196774	6299.505154	8.194982	-0.049114	4.290050
243.103935	6307.537832	8.199987	-0.049102	4.292687
243.378208	6315.586880	8.204992	-0.049158	4.295331
243.573858	6323.606633	8.209997	-0.049200	4.297963
244.006262	6331.596451	8.215002	-0.049285	4.300585
244.291068	6339.592761	8.220006	-0.049344	4.303207
244.219035	6347.586810	8.225011	-0.049335	4.305823
244.688547	6355.655749	8.230016	-0.049428	4.308466
244.677077	6363.666897	8.235021	-0.049431	4.311086
244.901730	6371.723637	8.240026	-0.049478	4.313720
245.274005	6379.729611	8.245030	-0.049552	4.316337
245.346850	6387.685783	8.250035	-0.049571	4.318935
245.716279	6395.718990	8.255040	-0.049645	4.321557
246.132114	6403.704525	8.260045	-0.049727	4.324163
246.451922	6411.730606	8.265050	-0.049792	4.326780
246.432807	6419.717847	8.270054	-0.049794	4.329380
246.579397	6427.749689	8.275059	-0.049826	4.331995
247.181144	6435.845415	8.280064	-0.049943	4.334631
247.304410	6443.856942	8.285069	-0.049971	4.337236
247.472621	6451.819564	8.290074	-0.050008	4.339823
248.000589	6459.871339	8.295078	-0.050111	4.342440
248.174419	6467.800308	8.300083	-0.050149	4.345013
248.344573	6475.873803	8.305088	-0.050186	4.347631
248.466022	6483.940640	8.310093	-0.050213	4.350246
248.685308	6492.003788	8.315098	-0.050259	4.352858
248.826314	6500.044388	8.320102	-0.050291	4.355461
248.855690	6508.002122	8.325107	-0.050301	4.358035
249.200743	6515.963635	8.330112	-0.050371	4.360610
249.470489	6523.973902	8.335117	-0.050426	4.363199
249.662466	6531.965284	8.340122	-0.050467	4.365780
249.994628	6540.017074	8.345126	-0.050534	4.368380
250.202479	6548.001402	8.350131	-0.050578	4.370955
250.100224	6556.052107	8.355136	-0.050564	4.373549
250.325368	6564.088379	8.360141	-0.050611	4.376138
250.758127	6572.059049	8.365146	-0.050697	4.378706
250.972461	6580.092598	8.370150	-0.050742	4.381292
250.934257	6588.076874	8.375155	-0.050740	4.383858
251.410205	6596.141017	8.380160	-0.050833	4.386452
251.452019	6604.130576	8.385165	-0.050846	4.389017
251.480728	6612.189271	8.390170	-0.050857	4.391604
251.741000	6620.196510	8.395174	-0.050910	4.394173
251.897088	6628.239396	8.400179	-0.050945	4.396752
252.204885	6636.216505	8.405184	-0.051007	4.399309
252.399135	6644.224492	8.410189	-0.051048	4.401873
252.419986	6652.170530	8.415194	-0.051057	4.404416
252.561694	6660.309826	8.420198	-0.051089	4.407019
252.789520	6668.230930	8.425203	-0.051136	4.409552
253.132782	6676.330042	8.430208	-0.051206	4.412140
253.369453	6684.306428	8.435213	-0.051255	4.414688
253.486484	6692.392957	8.440218	-0.051282	4.417268
253.803318	6700.385530	8.445222	-0.051346	4.419818
253.949380	6708.395950	8.450227	-0.051378	4.422371
254.066284	6716.383999	8.455232	-0.051405	4.424915
254.414800	6724.463916	8.460237	-0.051475	4.427488
254.653043	6732.448010	8.465242	-0.051525	4.430029
254.701632	6740.522712	8.470246	-0.051539	4.432596
254.737312	6748.543312	8.475251	-0.051551	4.435145
254.994911	6756.551045	8.480256	-0.051604	4.437689
255.100009	6764.468907	8.485261	-0.051628	4.440202
255.275253	6772.525352	8.490266	-0.051666	4.442758
255.440883	6780.521607	8.495270	-0.051702	4.445293
255.671660	6788.527658	8.500275	-0.051750	4.447830
255.811143	6796.554217	8.505280	-0.051781	4.450372
256.145252	6804.618773	8.510285	-0.051849	4.452926
256.394857	6812.619909	8.515290	-0.051900	4.455457
256.551416	6820.692905	8.520294	-0.051935	4.458009
256.887843	6828.626332	8.525299	-0.052002	4.460516
257.041720	6836.672106	8.530304	-0.052036	4.463057
257.167802	6844.627805	8.535309	-0.052065	4.465568
257.169931	6852.683359	8.540314	-0.052070	4.468108
257.559608	6860.724830	8.545318	-0.052148	4.470644
257.723278	6868.719673	8.550323	-0.052184	4.473163
257.897544	6876.763633	8.555328	-0.052221	4.475696
257.964692	6884.760614	8.560333	-0.052239	4.478212
258.150644	6892.744168	8.565338	-0.052279	4.480723
258.321243	6900.832778	8.570343	-0.052315	4.483266
258.434221	6908.767477	8.575347	-0.052342	4.485758
258.705607	6916.758025	8.580352	-0.052397	4.488267
259.107337	6924.821756	8.585357	-0.052477	4.490798
259.083470	6932.856790	8.590362	-0.052478	4.493318
259.549471	6940.888489	8.595367	-0.052570	4.495836
259.668679	6948.876697	8.600371	-0.052597	4.498338
259.906725	6956.909420	8.605376	-0.052647	4.500853
260.067209	6964.901387	8.610381	-0.052682	4.503354
260.339124	6972.928039	8.615386	-0.052737	4.505864
260.464823	6980.933310	8.620391	-0.052766	4.508366
260.584692	6988.935124	8.625395	-0.052793	4.510866
260.707196	6997.074471	8.630400	-0.052821	4.513407
261.050797	7005.046901	8.635405	-0.052890	4.515895
261.140290	7012.999381	8.640410	-0.052912	4.518375
261.437979	7021.020179	8.645415	-0.052973	4.520875
261.336033	7028.997692	8.650419	-0.052959	4.523359
261.798659	7037.035634	8.655424	-0.053050	4.525862
262.058048	7045.033123	8.660429	-0.053104	4.528351
262.167373	7053.030869	8.665434	-0.053129	4.530838
262.243105	7061.090504	8.670439	-0.053148	4.533342
262.178682	7069.133177	8.675443	-0.053142	4.535840
262.515459	7077.146255	8.680448	-0.053209	4.538328
262.754479	7085.140138	8.685453	-0.053259	4.540809
262.930032	7093.130699	8.690458	-0.053297	4.543287
263.250357	7101.151328	8.695463	-0.053362	4.545773
263.172608	7109.184022	8.700467	-0.053352	4.548261
263.457126	7117.217788	8.705472	-0.053410	4.550748
263.420211	7125.253109	8.710477	-0.053409	4.553234
263.560000	7133.244793	8.715482	-0.053440	4.555705
263.898793	7141.243321	8.720487	-0.053508	4.558178
264.138827	7149.239528	8.725491	-0.053558	4.560648
264.347432	7157.292854	8.730496	-0.053602	4.563134
264.181353	7165.315115	8.735501	-0.053576	4.565609
264.384276	7173.322641	8.740506	-0.053619	4.568079
264.723154	7181.312028	8.745511	-0.053687	4.570541
264.814591	7189.412752	8.750515	-0.053709	4.573037
264.898520	7197.413480	8.755520	-0.053730	4.575500
264.959524	7205.421637	8.760525	-0.053747	4.577964
265.372060	7213.376857	8.765530	-0.053829	4.580411
265.826937	7221.465489	8.770535	-0.053918	4.582897
265.761712	7229.415782	8.775539	-0.053911	4.585340
265.924091	7237.480004	8.780544	-0.053947	4.587816
266.141150	7245.505892	8.785549	-0.053992	4.590279
266.130503	7253.536231	8.790554	-0.053995	4.592742
266.472705	7261.563748	8.795559	-0.054064	4.595202
266.358049	7269.549758	8.800563	-0.054048	4.597649
266.786255	7277.511636	8.805568	-0.054133	4.600087
266.919522	7285.562435	8.810573	-0.054163	4.602551
267.026119	7293.523661	8.815578	-0.054188	4.604986
267.267172	7301.617987	8.820583	-0.054238	4.607461
267.413416	7309.576638	8.825587	-0.054270	4.609892
267.753404	7317.660486	8.830592	-0.054339	4.612361
267.650383	7325.675470	8.835597	-0.054325	4.614807
267.916802	7333.693278	8.840602	-0.054379	4.617253
268.344404	7341.677867	8.845607	-0.054464	4.619687
268.415976	7349.713216	8.850611	-0.054483	4.622136
268.717066	7357.652919	8.855616	-0.054544	4.624554
268.543765	7365.747524	8.860621	-0.054517	4.627018
268.875476	7373.718439	8.865626	-0.054584	4.629443
269.316672	7381.763827	8.870631	-0.054671	4.631889
269.441723	7389.752033	8.875635	-0.054699	4.634317
269.472857	7397.843893	8.880640	-0.054710	4.636775
269.684509	7405.775098	8.885645	-0.054755	4.639182
269.938488	7413.829023	8.890650	-0.054807	4.641626
270.346563	7421.778756	8.895655	-0.054888	4.644037
270.218335	7429.832570	8.900659	-0.054870	4.646478
270.599660	7437.827838	8.905664	-0.054946	4.648900
270.637248	7445.879509	8.910669	-0.054958	4.651338
270.601970	7453.851503	8.915674	-0.054956	4.653750
270.930805	7461.895487	8.920679	-0.055023	4.656183
271.129862	7469.892537	8.925683	-0.055065	4.658600
271.280331	7477.939043	8.930688	-0.055098	4.661031
271.485912	7485.950825	8.935693	-0.055141	4.663451
271.512434	7493.930662	8.940698	-0.055152	4.665859
271.822719	7502.012576	8.945703	-0.055214	4.668297
271.794390	7509.990109	8.950707	-0.055214	4.670702
272.007826	7518.077927	8.955712	-0.055259	4.673140
272.192555	7526.149137	8.960717	-0.055299	4.675570
272.165923	7534.045841	8.965722	-0.055299	4.677948
272.494568	7542.062121	8.970727	-0.055365	4.680359
272.673664	7550.028657	8.975731	-0.055404	4.682755
272.640464	7558.027937	8.980736	-0.055403	4.685159
272.964836	7566.097392	8.985741	-0.055468	4.687583
273.219334	7574.055186	8.990746	-0.055521	4.689972
273.234449	7582.157815	8.995751	-0.055529	4.692404
273.485868	7590.112486	9.000755	-0.055581	4.694789
273.683217	7598.178146	9.005760	-0.055623	4.697207
273.740517	7606.159325	9.010765	-0.055638	4.699598
274.130237	7614.203774	9.015770	-0.055716	4.702006
274.336522	7622.141349	9.020775	-0.055759	4.704382
274.486869	7630.162887	9.025779	-0.055793	4.706782
274.366132	7638.232032	9.030784	-0.055775	4.709195
274.599668	7646.258463	9.035789	-0.055824	4.711593
274.768144	7654.294730	9.040794	-0.055860	4.713993
275.095289	7662.342998	9.045799	-0.055927	4.716395
275.241678	7670.237776	9.050803	-0.055959	4.718751
275.350314	7678.297408	9.055808	-0.055984	4.721155
275.448838	7686.289863	9.060813	-0.056008	4.723537
275.360613	7694.299091	9.065818	-0.055996	4.725924
275.857722	7702.395208	9.070823	-0.056094	4.728333
275.982094	7710.360419	9.075827	-0.056122	4.730704
276.005006	7718.420913	9.080832	-0.056132	4.733102
276.115065	7726.456049	9.085837	-0.056157	4.735491
276.282113	7734.421353	9.090842	-0.056194	4.737858
276.365360	7742.429672	9.095847	-0.056214	4.740236
276.640435	7750.459076	9.100851	-0.056271	4.742619
276.771807	7758.460366	9.105856	-0.056300	4.744993
276.875334	7766.512755	9.110861	-0.056325	4.747381
277.056291	7774.471203	9.115866	-0.056363	4.749740
277.430325	7782.558401	9.120871	-0.056438	4.752135
277.527168	7790.574536	9.125875	-0.056461	4.754509
277.801885	7798.586514	9.130880	-0.056518	4.756879
277.841944	7806.583636	9.135885	-0.056530	4.759245
277.901950	7814.570246	9.140890	-0.056547	4.761606
278.283982	7822.557882	9.145895	-0.056623	4.763966
278.156263	7830.585866	9.150899	-0.056604	4.766338
278.585542	7838.592898	9.155904	-0.056689	4.768700
278.779008	7846.637728	9.160909	-0.056730	4.771074
278.827356	7854.609371	9.165914	-0.056745	4.773425
279.026420	7862.708999	9.170919	-0.056787	4.775812
279.185216	7870.659561	9.175923	-0.056821	4.778154
279.444887	7878.673932	9.180928	-0.056875	4.780513
279.591082	7886.721396	9.185933	-0.056907	4.782882
279.813311	7894.699799	9.190938	-0.056954	4.785228
280.242614	7902.752362	9.195943	-0.057039	4.787594
280.212852	7910.719974	9.200947	-0.057038	4.789936
280.423439	7918.805897	9.205952	-0.057083	4.792311
280.701923	7926.782174	9.210957	-0.057140	4.794652
280.436997	7934.819464	9.215962	-0.057096	4.797012
280.984007	7942.760273	9.220967	-0.057203	4.799339
281.061184	7950.826084	9.225971	-0.057222	4.801704
281.030280	7958.768327	9.230976	-0.057221	4.804031
281.100319	7966.867545	9.235981	-0.057240	4.806403
281.436303	7974.800525	9.240986	-0.057307	4.808724
281.543962	7982.899909	9.245991	-0.057333	4.811094
281.905868	7990.372633	9.250995	-0.057405	4.813278
282.140651	7994.921283	9.256000	-0.057451	4.814607

282.272660	7997.396090	9.261005	-0.057477	4.815329
282.093353	7998.673532	9.266010	-0.057445	4.815704
282.348990	7999.322264	9.271015	-0.057493	4.815892
282.456828	7999.735476	9.276019	-0.057513	4.816012
282.561556	7999.802526	9.281024	-0.057532	4.816031
282.772001	7999.814872	9.286029	-0.057572	4.816034
282.981503	7999.715034	9.291034	-0.057610	4.816003
282.934170	7999.761172	9.296039	-0.057602	4.816017
282.871313	7999.781391	9.301043	-0.057590	4.816023
282.784004	7999.781939	9.306048	-0.057573	4.816024
283.005939	7999.812654	9.311053	-0.057615	4.816032
283.148411	7999.851545	9.316058	-0.057641	4.816042
283.197149	7999.844941	9.321063	-0.057650	4.816040
283.375051	7999.993439	9.326067	-0.057683	4.816083
283.388924	7999.895400	9.331072	-0.057686	4.816054
283.498486	7999.831142	9.336077	-0.057706	4.816035
283.310249	7999.977284	9.341082	-0.057671	4.816078
283.533088	7999.839229	9.346087	-0.057712	4.816037
283.441180	7999.918745	9.351091	-0.057695	4.816060
283.558713	7999.904840	9.356096	-0.057717	4.816056
283.647670	7999.904306	9.361101	-0.057733	4.816055
283.756285	7999.878489	9.366106	-0.057753	4.816047
283.814808	7999.822920	9.371111	-0.057764	4.816030
283.952682	7999.955740	9.376115	-0.057790	4.816069
283.920939	7999.918835	9.381120	-0.057784	4.816058
283.744221	7999.925240	9.386125	-0.057751	4.816061
283.881473	7999.913829	9.391130	-0.057776	4.816057
283.914256	7999.869546	9.396135	-0.057782	4.816044
283.698306	7999.909426	9.401139	-0.057742	4.816056
283.873012	7999.923264	9.406144	-0.057774	4.816059
283.892506	7999.828531	9.411149	-0.057778	4.816032
283.900818	7999.986780	9.416154	-0.057780	4.816078
283.937131	7999.884872	9.421159	-0.057786	4.816048
284.170237	7999.927544	9.426163	-0.057829	4.816059
284.117959	7999.904154	9.431168	-0.057820	4.816053
284.202339	7999.916357	9.436173	-0.057835	4.816056
283.963314	7999.984663	9.441178	-0.057791	4.816077
284.130624	7999.880855	9.446183	-0.057822	4.816046
284.048708	7999.972305	9.451187	-0.057806	4.816073
284.099009	7999.893084	9.456192	-0.057816	4.816049
284.370508	7999.902267	9.461197	-0.057866	4.816051
284.261014	7999.916299	9.466202	-0.057846	4.816055
284.142182	7999.873542	9.471207	-0.057823	4.816044
284.183880	7999.894587	9.476211	-0.057831	4.816049
284.267462	7999.835199	9.481216	-0.057847	4.816032
284.261104	7999.963271	9.486221	-0.057845	4.816069
284.176182	7999.888011	9.491226	-0.057829	4.816048
284.533554	7999.838924	9.496231	-0.057896	4.816031
284.262830	7999.929090	9.501235	-0.057845	4.816059
284.215826	7999.881225	9.506240	-0.057836	4.816045
284.507987	7999.930309	9.511245	-0.057891	4.816058
284.317821	7999.893738	9.516250	-0.057855	4.816049
284.388541	7999.916376	9.521255	-0.057868	4.816055
284.359205	7999.932929	9.526259	-0.057863	4.816060
284.477558	7999.879512	9.531264	-0.057885	4.816044
284.566156	7999.914226	9.536269	-0.057901	4.816053
284.444959	7999.993213	9.541274	-0.057879	4.816077
284.646804	7999.813112	9.546279	-0.057916	4.816023
284.526652	8000.050228	9.551283	-0.057894	4.816093
284.343219	7999.879172	9.556288	-0.057859	4.816044
284.591474	7999.934939	9.561293	-0.057905	4.816059
284.452950	7999.949513	9.566298	-0.057880	4.816064
284.556023	7999.905435	9.571303	-0.057899	4.816051
284.475105	7999.995835	9.576307	-0.057884	4.816078
284.593978	7999.876192	9.581312	-0.057906	4.816042
284.816471	7999.927220	9.586317	-0.057947	4.816056
284.745646	7999.881059	9.591322	-0.057934	4.816043
284.947275	7999.912479	9.596327	-0.057971	4.816051
285.005959	7999.923148	9.601331	-0.057982	4.816054
284.886578	7999.910293	9.606336	-0.057960	4.816050
284.884830	7999.911321	9.611341	-0.057959	4.816051
284.999227	7999.805485	9.616346	-0.057980	4.816019
285.054507	7999.965658	9.621351	-0.057991	4.816066
284.854038	7999.848775	9.626355	-0.057953	4.816033
284.819673	7999.932541	9.631360	-0.057947	4.816057
284.687185	7999.816891	9.636365	-0.057922	4.816024
284.858167	8000.003730	9.641370	-0.057954	4.816078
284.972744	7999.869052	9.646375	-0.057975	4.816038
284.960537	7999.909418	9.651379	-0.057973	4.816050
285.019973	7999.892325	9.656384	-0.057984	4.816045
284.923873	7999.949332	9.661389	-0.057966	4.816062
285.117216	7999.997697	9.666394	-0.058002	4.816075
284.967382	7999.882799	9.671399	-0.057973	4.816042
284.979085	7999.910779	9.676403	-0.057976	4.816050
284.990638	7999.846880	9.681408	-0.057978	4.816031
284.973214	7999.933090	9.686413	-0.057974	4.816057
285.117258	7999.979492	9.691418	-0.058001	4.816069
285.297301	7999.883391	9.696423	-0.058034	4.816040
285.091163	7999.911697	9.701427	-0.057996	4.816050
285.242744	7999.833243	9.706432	-0.058024	4.816026
285.297836	7999.859872	9.711437	-0.058034	4.816034
285.067796	7999.920863	9.716442	-0.057991	4.816053
285.121668	7999.959221	9.721447	-0.058001	4.816064
285.161491	7999.857375	9.726451	-0.058009	4.816034
285.238442	7999.858761	9.731456	-0.058023	4.816034
285.316340	7999.963791	9.736461	-0.058037	4.816064
285.096980	7999.825199	9.741466	-0.057996	4.816025
285.228772	7999.921590	9.746471	-0.058021	4.816052
285.218530	7999.932079	9.751475	-0.058019	4.816055
285.047657	7999.885173	9.756480	-0.057987	4.816042
285.081458	7999.901802	9.761485	-0.057993	4.816047
285.115723	7999.905619	9.766490	-0.057999	4.816048
285.177559	7999.929165	9.771495	-0.058011	4.816054
285.155191	7999.930888	9.776499	-0.058007	4.816055
285.054488	7999.895936	9.781504	-0.057988	4.816045
285.251086	7999.897353	9.786509	-0.058024	4.816045
285.012424	8000.086387	9.791514	-0.057980	4.816101
285.083473	7999.902845	9.796519	-0.057993	4.816047
285.211418	7999.998099	9.801523	-0.058017	4.816074
285.195981	7999.995674	9.806528	-0.058014	4.816074
285.310311	7999.909066	9.811533	-0.058035	4.816048
285.289208	7999.983458	9.816538	-0.058031	4.816070
285.256851	7999.882440	9.821543	-0.058025	4.816040
285.231167	7999.903332	9.826547	-0.058020	4.816047
285.389280	7999.964947	9.831552	-0.058049	4.816064
285.548495	7999.823598	9.836557	-0.058079	4.816022
285.292124	8000.004833	9.841562	-0.058031	4.816076
285.411532	7999.896950	9.846567	-0.058053	4.816044
285.509546	7999.891239	9.851571	-0.058071	4.816042
285.463028	7999.981196	9.856576	-0.058062	4.816068
285.577549	7999.929846	9.861581	-0.058084	4.816053
285.505512	7999.983017	9.866586	-0.058070	4.816069
285.525706	7999.897907	9.871591	-0.058074	4.816044
285.396733	7999.938295	9.876595	-0.058050	4.816056
285.381292	7999.869633	9.881600	-0.058047	4.816036
285.405595	7999.950189	9.886605	-0.058051	4.816059
285.211516	7999.969098	9.891610	-0.058015	4.816066
285.491057	7999.903646	9.896615	-0.058067	4.816045
285.607535	7999.914294	9.901619	-0.058089	4.816048
285.437331	7999.885561	9.906624	-0.058057	4.816040
285.312733	7999.828810	9.911629	-0.058033	4.816025
285.364082	7999.884216	9.916634	-0.058043	4.816040
285.440221	7999.915501	9.921639	-0.058057	4.816049
285.259420	7999.928240	9.926643	-0.058023	4.816054
285.285051	7999.891305	9.931648	-0.058028	4.816043
285.574854	7999.873044	9.936653	-0.058082	4.816036
285.469155	7999.925605	9.941658	-0.058062	4.816052
285.378709	7999.849174	9.946663	-0.058045	4.816030
285.375000	7999.938838	9.951667	-0.058044	4.816056
285.581292	7999.873126	9.956672	-0.058083	4.816036
285.562049	7999.917638	9.961677	-0.058079	4.816049
285.338180	7999.989424	9.966682	-0.058037	4.816071
285.754576	7999.850600	9.971687	-0.058115	4.816029
285.514267	7999.918883	9.976691	-0.058070	4.816050
285.589586	7999.825157	9.981696	-0.058084	4.816022
285.847335	7999.930243	9.986701	-0.058132	4.816051
285.471275	7999.876413	9.991706	-0.058062	4.816038
285.490863	7999.852187	9.996711	-0.058065	4.816030
285.798932	7999.944296	10.001715	-0.058122	4.816056
285.544214	7999.847795	10.006720	-0.058075	4.816029
285.530376	7999.935138	10.011725	-0.058072	4.816054
285.490418	7999.842529	10.016730	-0.058065	4.816028
285.598341	7999.864774	10.021735	-0.058085	4.816034
285.766008	7999.928699	10.026739	-0.058116	4.816051
285.699038	7999.814233	10.031744	-0.058103	4.816018
285.656125	7999.967287	10.036749	-0.058095	4.816063
285.489427	7999.812554	10.041754	-0.058064	4.816019
285.459130	7999.894258	10.046759	-0.058058	4.816043
285.555785	7999.962237	10.051763	-0.058076	4.816062
285.461581	7999.888943	10.056768	-0.058059	4.816041
285.545340	7999.869085	10.061773	-0.058074	4.816035
285.522051	7999.916730	10.066778	-0.058070	4.816049
285.633230	7999.817244	10.071783	-0.058090	4.816020
285.660119	7999.922419	10.076787	-0.058095	4.816050
285.478135	7999.861423	10.081792	-0.058061	4.816033
285.678323	7999.907775	10.086797	-0.058098	4.816046
285.634635	7999.975348	10.091802	-0.058090	4.816066
285.651909	7999.878434	10.096807	-0.058093	4.816037
285.678851	7999.856478	10.101811	-0.058098	4.816031
285.634272	7999.886643	10.106816	-0.058090	4.816040
285.732525	7999.924739	10.111821	-0.058108	4.816050
285.583784	7999.909214	10.116826	-0.058080	4.816047
285.680330	7999.858607	10.121831	-0.058098	4.816031
285.767741	7999.947786	10.126835	-0.058114	4.816057
285.561895	7999.788070	10.131840	-0.058076	4.816011
285.721422	7999.939450	10.136845	-0.058106	4.816055
285.733372	7999.822141	10.141850	-0.058108	4.816020
285.762335	7999.918807	10.146855	-0.058113	4.816049
285.779089	7999.910556	10.151859	-0.058116	4.816046
285.861594	7999.829780	10.156864	-0.058131	4.816022
285.795137	7999.868096	10.161869	-0.058119	4.816034
285.738875	7999.935441	10.166874	-0.058108	4.816054
286.066460	7999.863380	10.171879	-0.058169	4.816031
286.029751	7999.860569	10.176883	-0.058162	4.816030
285.664754	7999.909499	10.181888	-0.058094	4.816046
285.878444	7999.870630	10.186893	-0.058134	4.816034
286.031257	7999.926808	10.191898	-0.058162	4.816049
285.783335	7999.849659	10.196903	-0.058116	4.816028
285.795442	7999.949225	10.201907	-0.058118	4.816057
285.878175	7999.810763	10.206912	-0.058133	4.816016
285.879287	7999.937907	10.211917	-0.058134	4.816054
285.651582	7999.833348	10.216922	-0.058091	4.816024
285.846482	7999.923406	10.221927	-0.058127	4.816049
285.885219	7999.832222	10.226931	-0.058134	4.816023
285.880949	7999.925082	10.231936	-0.058134	4.816050
285.821472	7999.833186	10.236941	-0.058122	4.816023
285.935091	7999.912157	10.241946	-0.058143	4.816046
285.869311	7999.854334	10.246951	-0.058131	4.816029
285.820025	7999.957061	10.251955	-0.058122	4.816059
286.019067	7999.844211	10.256960	-0.058159	4.816025
286.071812	7999.919942	10.261965	-0.058168	4.816047
285.711271	7999.855709	10.266970	-0.058101	4.816030
285.872853	7999.906703	10.271975	-0.058131	4.816045
285.928408	7999.875651	10.276979	-0.058141	4.816035
285.708503	7999.848154	10.281984	-0.058100	4.816028
285.958947	7999.877255	10.286989	-0.058147	4.816035
285.994526	7999.939855	10.291994	-0.058154	4.816054
285.938027	7999.872585	10.296999	-0.058143	4.816034
285.922938	7999.815681	10.302003	-0.058140	4.816018
285.820416	7999.970860	10.307008	-0.058121	4.816064
285.981705	7999.835959	10.312013	-0.058151	4.816023
286.044619	7999.978112	10.317018	-0.058162	4.816064
285.901604	7999.793893	10.322023	-0.058136	4.816011
285.912611	7999.923353	10.327027	-0.058138	4.816049
285.891657	7999.872752	10.332032	-0.058134	4.816035
286.117966	7999.836248	10.337037	-0.058176	4.816023
286.204742	7999.905118	10.342042	-0.058192	4.816042
286.062718	7999.908945	10.347047	-0.058165	4.816044
286.001572	7999.859752	10.352051	-0.058154	4.816030
286.019599	7999.914556	10.357056	-0.058157	4.816046
286.183212	7999.871574	10.362061	-0.058187	4.816033
286.184766	7999.932489	10.367066	-0.058188	4.816050
286.133016	7999.870646	10.372071	-0.058178	4.816033
286.050003	7999.848835	10.377075	-0.058162	4.816027
286.139547	7999.830150	10.382080	-0.058179	4.816021
286.092293	7999.958555	10.387085	-0.058170	4.816059
285.957765	7999.856752	10.392090	-0.058145	4.816030
285.939716	7999.844664	10.397095	-0.058141	4.816026
286.008385	7999.951666	10.402099	-0.058154	4.816057
285.908033	7999.816296	10.407104	-0.058135	4.816018
286.050727	7999.949211	10.412109	-0.058162	4.816056
285.738302	7999.902943	10.417114	-0.058104	4.816044
285.815608	7999.862670	10.422119	-0.058118	4.816032
286.180446	7999.866068	10.427123	-0.058186	4.816031
286.080611	7999.845020	10.432128	-0.058167	4.816025
286.080780	7999.994582	10.437133	-0.058167	4.816069
286.220239	7999.868900	10.442138	-0.058193	4.816032
286.226257	7999.821993	10.447143	-0.058194	4.816018
286.112209	7999.902180	10.452147	-0.058173	4.816042
286.243641	7999.944082	10.457152	-0.058197	4.816054
286.356182	7999.904448	10.462157	-0.058218	4.816041
286.179797	7999.860645	10.467162	-0.058185	4.816030
286.194052	7999.892945	10.472167	-0.058187	4.816039
286.287031	7999.903168	10.477171	-0.058205	4.816041
286.075493	7999.857659	10.482176	-0.058165	4.816029
286.014160	7999.899273	10.487181	-0.058154	4.816042
286.022143	7999.919707	10.492186	-0.058155	4.816048
286.287942	7999.888193	10.497191	-0.058204	4.816037
286.339392	7999.862408	10.502195	-0.058214	4.816029
286.192448	7999.917426	10.507200	-0.058187	4.816046
286.328989	7999.847245	10.512205	-0.058212	4.816025
286.204079	7999.864202	10.517210	-0.058189	4.816030
286.082014	7999.861981	10.522215	-0.058166	4.816030
286.243401	7999.878786	10.527219	-0.058196	4.816035
286.187154	7999.956815	10.532224	-0.058185	4.816058
286.212800	7999.885692	10.537229	-0.058190	4.816037
286.219454	7999.859095	10.542234	-0.058191	4.816029
286.391436	7999.857930	10.547239	-0.058223	4.816028
286.350161	7999.872130	10.552243	-0.058215	4.816032
286.221787	7999.965946	10.557248	-0.058191	4.816060
286.397735	7999.864428	10.562253	-0.058224	4.816030
286.316870	7999.842655	10.567258	-0.058209	4.816024
286.327184	7999.893046	10.572263	-0.058210	4.816038
286.299303	7999.882917	10.577267	-0.058205	4.816035
286.229969	7999.927590	10.582272	-0.058192	4.816049
286.510516	7999.881386	10.587277	-0.058244	4.816034
286.470578	7999.910567	10.592282	-0.058237	4.816043
286.617811	7999.936731	10.597287	-0.058264	4.816049
286.377397	7999.922749	10.602291	-0.058219	4.816047
286.352196	7999.873139	10.607296	-0.058214	4.816032
286.580919	7999.910396	10.612301	-0.058257	4.816042
286.140494	7999.892788	10.617306	-0.058175	4.816039
286.105390	7999.895348	10.622311	-0.058168	4.816040
286.205058	7999.940948	10.627315	-0.058187	4.816053
286.266669	7999.864067	10.632320	-0.058198	4.816030
286.267593	7999.895057	10.637325	-0.058198	4.816039
286.235544	7999.856007	10.642330	-0.058192	4.816028
286.334646	7999.898392	10.647335	-0.058210	4.816040
286.300351	7999.984298	10.652339	-0.058204	4.816065
286.246749	7999.845500	10.657344	-0.058194	4.816025
286.510340	7999.883388	10.662349	-0.058243	4.816035
286.295610	7999.829275	10.667354	-0.058203	4.816020
286.261828	7999.940830	10.672359	-0.058197	4.816053
286.410202	7999.850565	10.677363	-0.058224	4.816025
286.554464	7999.827530	10.682368	-0.058251	4.816018
286.609481	7999.875526	10.687373	-0.058261	4.816032
286.461006	7999.948679	10.692378	-0.058233	4.816054
286.587158	7999.897540	10.697383	-0.058257	4.816038
286.647594	7999.916789	10.702387	-0.058268	4.816044
286.465415	7999.851513	10.707392	-0.058234	4.816025
286.647860	7999.914639	10.712397	-0.058268	4.816043
286.376826	7999.876598	10.717402	-0.058217	4.816033
286.541962	7999.877446	10.722407	-0.058248	4.816033
286.445817	7999.947274	10.727411	-0.058230	4.816054
286.387196	7999.857530	10.732416	-0.058219	4.816028
286.444425	7999.894882	10.737421	-0.058229	4.816038
286.462924	7999.859953	10.742426	-0.058233	4.816028
286.601089	7999.849629	10.747431	-0.058258	4.816024
286.598548	7999.890171	10.752435	-0.058258	4.816036
286.549389	7999.829444	10.757440	-0.058248	4.816019
286.522238	7999.902659	10.762445	-0.058243	4.816040
286.623911	7999.936544	10.767450	-0.058262	4.816049
286.486143	7999.869937	10.772455	-0.058236	4.816031
286.505286	7999.875617	10.777459	-0.058240	4.816032
286.408287	7999.852483	10.782464	-0.058222	4.816026
286.276320	7999.902431	10.787469	-0.058197	4.816041
286.402521	7999.979495	10.792474	-0.058221	4.816063
286.363050	7999.837748	10.797479	-0.058213	4.816022
286.662370	7999.877352	10.802483	-0.058269	4.816032
286.330821	7999.838215	10.807488	-0.058207	4.816022
286.493259	7999.876406	10.812493	-0.058237	4.816033
286.635586	7999.979403	10.817498	-0.058264	4.816062
286.468957	7999.872743	10.822503	-0.058232	4.816032
286.397436	7999.883189	10.827507	-0.058219	4.816035
286.364930	7999.847336	10.832512	-0.058213	4.816025
286.631781	7999.889557	10.837517	-0.058262	4.816036
286.571720	7999.867092	10.842522	-0.058251	4.816030
286.530097	7999.898379	10.847527	-0.058243	4.816039
286.517141	7999.890657	10.852531	-0.058241	4.816037
286.187071	7999.923126	10.857536	-0.058179	4.816048
286.352522	7999.879109	10.862541	-0.058210	4.816034
286.506873	7999.870146	10.867546	-0.058239	4.816031
286.419676	7999.868557	10.872551	-0.058222	4.816031
286.540476	7999.901720	10.877555	-0.058245	4.816040
286.531311	7999.903682	10.882560	-0.058243	4.816040
286.807773	7999.902275	10.887565	-0.058294	4.816039
286.657954	7999.865363	10.892570	-0.058266	4.816029
286.587650	7999.924976	10.897575	-0.058253	4.816046
286.424935	7999.934837	10.902579	-0.058223	4.816050
286.287639	7999.905631	10.907584	-0.058197	4.816042
286.447285	7999.933088	10.912589	-0.058227	4.816049
286.445433	7999.896722	10.917594	-0.058226	4.816039
286.423274	7999.928362	10.922599	-0.058222	4.816048
286.489623	7999.897506	10.927603	-0.058234	4.816039
286.496027	7999.845264	10.932608	-0.058235	4.816024
286.622561	7999.909513	10.937613	-0.058259	4.816042
286.485889	7999.866429	10.942618	-0.058233	4.816030
286.359213	7999.916474	10.947623	-0.058210	4.816045
286.325405	7999.968201	10.952627	-0.058203	4.816060
286.481421	7999.895168	10.957632	-0.058232	4.816038
286.461909	7999.874506	10.962637	-0.058229	4.816032
286.301384	7999.969876	10.967642	-0.058199	4.816061
286.486886	7999.908061	10.972647	-0.058233	4.816042
286.614520	7999.912502	10.977651	-0.058257	4.816043
286.657992	7999.831018	10.982656	-0.058265	4.816019
286.659575	7999.883388	10.987661	-0.058265	4.816034
286.446854	7999.853882	10.992666	-0.058225	4.816026
286.496288	7999.835539	10.997671	-0.058234	4.816021
286.534502	7999.901393	11.002675	-0.058241	4.816040
286.573756	7999.887139	11.007680	-0.058249	4.816035
286.721262	7999.865232	11.012685	-0.058276	4.816028
286.700511	7999.973819	11.017690	-0.058272	4.816060
286.808157	7999.895635	11.022695	-0.058292	4.816037
286.686941	7999.890224	11.027699	-0.058269	4.816036
286.386540	7999.874086	11.032704	-0.058213	4.816033
286.568753	7999.868833	11.037709	-0.058247	4.816030
286.487712	7999.889791	11.042714	-0.058232	4.816037
286.472957	7999.947206	11.047719	-0.058229	4.816054
286.626226	7999.910447	11.052723	-0.058258	4.816042
286.535185	7999.884215	11.057728	-0.058240	4.816035
286.357841	7999.897017	11.062733	-0.058207	4.816040
286.492957	7999.889842	11.067738	-0.058232	4.816037
286.462898	7999.918134	11.072743	-0.058227	4.816045
286.643285	7999.880798	11.077747	-0.058260	4.816033
286.566757	7999.869787	11.082752	-0.058246	4.816030
286.727886	7999.922912	11.087757	-0.058276	4.816045
286.538117	7999.892754	11.092762	-0.058240	4.816037
286.554187	7999.922950	11.097767	-0.058243	4.816046
286.609039	7999.905774	11.102771	-0.058253	4.816041
286.459704	7999.895580	11.107776	-0.058226	4.816039
286.379812	7999.925105	11.112781	-0.058211	4.816048
286.449656	7999.921020	11.117786	-0.058223	4.816046
286.616978	7999.888789	11.122791	-0.058255	4.816036
286.560502	7999.927286	11.127795	-0.058244	4.816047
286.318688	7999.841699	11.132800	-0.058199	4.816024
286.495074	7999.899373	11.137805	-0.058232	4.816040
286.591890	7999.898983	11.142810	-0.058249	4.816039
286.506672	7999.863242	11.147815	-0.058234	4.816029
286.772344	7999.897963	11.152819	-0.058283	4.816038
286.730703	7999.942071	11.157824	-0.058275	4.816051
286.682595	7999.865336	11.162829	-0.058266	4.816029
286.573909	7999.940279	11.167834	-0.058246	4.816051
286.672525	7999.867273	11.172839	-0.058264	4.816029
286.579029	7999.898688	11.177843	-0.058246	4.816039
286.581510	7999.851717	11.182848	-0.058247	4.816025
286.907786	7999.884332	11.187853	-0.058307	4.816033
286.810230	7999.878281	11.192858	-0.058289	4.816032
286.507389	7999.893081	11.197863	-0.058233	4.816038
286.659679	7999.934294	11.202867	-0.058261	4.816049
286.672343	7999.867208	11.207872	-0.058263	4.816029
286.689427	7999.854689	11.212877	-0.058266	4.816025
286.694218	7999.956261	11.217882	-0.058267	4.816055
286.831290	7999.883952	11.222887	-0.058293	4.816033
286.792658	7999.929183	11.227891	-0.058285	4.816047
286.549160	7999.875615	11.232896	-0.058240	4.816032
286.857386	7999.892946	11.237901	-0.058297	4.816036
286.896902	7999.871218	11.242906	-0.058304	4.816029
286.804282	7999.862052	11.247911	-0.058287	4.816027
286.778015	7999.914985	11.252915	-0.058282	4.816043
286.768509	7999.849634	11.257920	-0.058280	4.816024
286.687154	7999.893021	11.262925	-0.058265	4.816037
286.789875	7999.941883	11.267930	-0.058284	4.816050
286.993697	7999.938091	11.272935	-0.058322	4.816048
286.846337	7999.917248	11.277939	-0.058294	4.816043
286.698509	7999.865415	11.282944	-0.058267	4.816029
286.885460	7999.883752	11.287949	-0.058302	4.816033
287.056510	7999.871888	11.292954	-0.058333	4.816029
286.940881	7999.879398	11.297959	-0.058312	4.816031
286.865286	7999.909001	11.302963	-0.058298	4.816040
286.834303	7999.849671	11.307968	-0.058292	4.816023
286.563714	7999.901379	11.312973	-0.058241	4.816040
286.802860	7999.872587	11.317978	-0.058286	4.816030
286.884631	7999.851625	11.322983	-0.058301	4.816024
286.764014	7999.907121	11.327987	-0.058278	4.816040
286.687546	7999.849103	11.332992	-0.058264	4.816024
286.883501	7999.869740	11.337997	-0.058300	4.816029
286.925502	7999.893997	11.343002	-0.058308	4.816036
286.628275	7999.891805	11.348007	-0.058253	4.816037
286.892020	7999.893373	11.353011	-0.058302	4.816036
286.924796	7999.955923	11.358016	-0.058308	4.816054
286.949106	7999.854861	11.363021	-0.058312	4.816024
286.861512	7999.861811	11.368026	-0.058296	4.816027
286.913389	7999.826418	11.373031	-0.058305	4.816016
286.927229	7999.895036	11.378035	-0.058308	4.816036
286.775079	7999.858081	11.383040	-0.058279	4.816026
286.929247	7999.871551	11.388045	-0.058308	4.816029
287.013208	7999.966012	11.393050	-0.058323	4.816056
286.812466	7999.874758	11.398055	-0.058286	4.816031
287.142892	7999.866851	11.403059	-0.058347	4.816027
286.968258	7999.854061	11.408064	-0.058315	4.816024
286.980051	7999.901274	11.413069	-0.058317	4.816038
286.808481	7999.866104	11.418074	-0.058285	4.816028
286.990904	7999.905726	11.423079	-0.058319	4.816039
287.082129	7999.886004	11.428083	-0.058336	4.816033
287.009526	7999.831261	11.433088	-0.058322	4.816017
286.909695	7999.883929	11.438093	-0.058303	4.816033
287.021394	7999.867783	11.443098	-0.058324	4.816028
286.861553	7999.827484	11.448103	-0.058294	4.816017
286.945686	7999.872803	11.453107	-0.058310	4.816030
287.145317	7999.943721	11.458112	-0.058347	4.816049
287.085075	7999.860356	11.463117	-0.058336	4.816025
287.075020	7999.877258	11.468122	-0.058334	4.816030
286.902025	7999.845268	11.473127	-0.058301	4.816022
287.035557	7999.878662	11.478131	-0.058326	4.816031
287.045489	7999.828620	11.483136	-0.058328	4.816016
287.230217	7999.913157	11.488141	-0.058362	4.816040
287.214503	7999.885086	11.493146	-0.058359	4.816032
287.059865	7999.848085	11.498151	-0.058330	4.816022
287.047500	7999.895929	11.503155	-0.058328	4.816036
286.885901	7999.946408	11.508160	-0.058298	4.816051
286.920387	7999.842325	11.513165	-0.058304	4.816021
287.034447	7999.847589	11.518170	-0.058325	4.816022
287.113135	7999.839392	11.523175	-0.058340	4.816019
287.071063	7999.954004	11.528179	-0.058332	4.816053
286.964952	7999.862329	11.533184	-0.058312	4.816026
287.134213	7999.860047	11.538189	-0.058343	4.816025
287.147442	7999.878440	11.543194	-0.058346	4.816030
287.074346	7999.852534	11.548199	-0.058332	4.816023
287.195188	7999.858989	11.553203	-0.058354	4.816024
286.986378	7999.849853	11.558208	-0.058315	4.816023
287.063228	7999.947391	11.563213	-0.058330	4.816051
287.082535	7999.861194	11.568218	-0.058333	4.816025
286.920569	7999.799489	11.573223	-0.058303	4.816008
287.080073	7999.912414	11.578227	-0.058333	4.816040
286.882098	7999.884243	11.583232	-0.058296	4.816033
287.175808	7999.872465	11.588237	-0.058350	4.816028
287.054581	7999.810430	11.593242	-0.058327	4.816011
286.951097	7999.903630	11.598247	-0.058308	4.816039
286.933819	7999.880872	11.603251	-0.058305	4.816032
287.069529	7999.838453	11.608256	-0.058330	4.816019
286.909625	7999.906057	11.613261	-0.058300	4.816040
286.901406	7999.884532	11.618266	-0.058299	4.816033
286.762841	7999.836072	11.623271	-0.058273	4.816020
286.934658	7999.881912	11.628275	-0.058305	4.816032
286.957337	7999.902613	11.633280	-0.058309	4.816038
287.154231	7999.834594	11.638285	-0.058345	4.816017
287.094170	7999.857000	11.643290	-0.058334	4.816024
286.863232	7999.890197	11.648295	-0.058291	4.816035
286.982928	7999.849624	11.653299	-0.058313	4.816023
287.001794	7999.829659	11.658304	-0.058317	4.816017
287.050479	7999.927754	11.663309	-0.058326	4.816045
287.128440	7999.902449	11.668314	-0.058340	4.816037
287.077057	7999.833133	11.673319	-0.058330	4.816017
287.312207	7999.860892	11.678323	-0.058374	4.816024
287.107342	7999.907382	11.683328	-0.058336	4.816039
287.179573	7999.834966	11.688333	-0.058349	4.816017
287.264252	7999.858928	11.693338	-0.058365	4.816024
287.223060	7999.872061	11.698343	-0.058357	4.816028
287.248269	7999.881056	11.703347	-0.058362	4.816030
287.103956	7999.888046	11.708352	-0.058335	4.816033
287.274639	7999.898611	11.713357	-0.058366	4.816035
287.243124	7999.901236	11.718362	-0.058360	4.816036
287.088486	7999.953978	11.723367	-0.058332	4.816053
287.143585	7999.926123	11.728371	-0.058342	4.816044
287.018380	7999.877904	11.733376	-0.058318	4.816031
287.022081	7999.849117	11.738381	-0.058319	4.816022
287.068932	7999.917264	11.743386	-0.058328	4.816042
287.072147	7999.885263	11.748391	-0.058328	4.816033
286.958899	7999.886406	11.753395	-0.058307	4.816034
287.034956	7999.918759	11.758400	-0.058321	4.816043
287.212236	7999.795897	11.763405	-0.058354	4.816006
287.205770	7999.887651	11.768410	-0.058353	4.816033
286.978155	7999.839712	11.773415	-0.058310	4.816020
286.908719	7999.898273	11.778419	-0.058297	4.816037
287.141563	7999.888597	11.783424	-0.058340	4.816033
287.191288	7999.839276	11.788429	-0.058349	4.816019
287.269122	7999.872730	11.793434	-0.058364	4.816028
287.190787	7999.861686	11.798439	-0.058349	4.816025
287.146859	7999.877974	11.803443	-0.058341	4.816030
287.207471	7999.921799	11.808448	-0.058352	4.816043
287.310525	7999.793318	11.813453	-0.058371	4.816005
287.136187	7999.942925	11.818458	-0.058339	4.816049
287.102655	7999.900642	11.823463	-0.058332	4.816037
287.273820	7999.863139	11.828467	-0.058364	4.816025
287.109743	7999.843061	11.833472	-0.058333	4.816020
287.147298	7999.872579	11.838477	-0.058340	4.816029
287.233998	7999.902988	11.843482	-0.058356	4.816037
287.230245	7999.885818	11.848487	-0.058356	4.816032
287.371898	7999.896924	11.853491	-0.058382	4.816035
287.124853	7999.936239	11.858496	-0.058336	4.816047
287.158134	7999.809698	11.863501	-0.058342	4.816010
287.317885	7999.934380	11.868506	-0.058372	4.816046
287.220370	7999.826835	11.873511	-0.058353	4.816015
287.171023	7999.931699	11.878515	-0.058344	4.816046
286.937424	7999.827029	11.883520	-0.058300	4.816016
287.006284	7999.834679	11.888525	-0.058313	4.816018
286.986667	7999.866365	11.893530	-0.058309	4.816028
287.087786	7999.946181	11.898535	-0.058328	4.816050
287.399755	7999.912299	11.903539	-0.058386	4.816039
287.394366	7999.883346	11.908544	-0.058385	4.816030
287.341917	7999.871703	11.913549	-0.058375	4.816027
287.430162	7999.849790	11.918554	-0.058392	4.816020
287.197566	7999.900051	11.923559	-0.058348	4.816036
287.129979	7999.864629	11.928563	-0.058336	4.816026
287.167504	7999.827908	11.933568	-0.058342	4.816015
287.169035	7999.857841	11.938573	-0.058343	4.816024
287.309509	7999.951191	11.943578	-0.058369	4.816051
287.385861	7999.824362	11.948583	-0.058383	4.816013
287.425374	7999.841095	11.953587	-0.058390	4.816018
287.069833	7999.972459	11.958592	-0.058324	4.816058
287.253685	7999.880699	11.963597	-0.058358	4.816030
287.346496	7999.886647	11.968602	-0.058375	4.816032
287.229989	7999.831107	11.973607	-0.058353	4.816016
287.255942	7999.881782	11.978611	-0.058358	4.816031
287.225480	7999.838487	11.983616	-0.058352	4.816018
287.391702	7999.903457	11.988621	-0.058383	4.816036
287.365561	7999.860239	11.993626	-0.058378	4.816024
287.289097	7999.823588	11.998631	-0.058364	4.816014
287.482863	7999.870896	12.003635	-0.058400	4.816026
287.222472	7999.905695	12.008640	-0.058351	4.816038
287.341869	7999.838407	12.013645	-0.058373	4.816018
287.471584	7999.899511	12.018650	-0.058398	4.816035
287.204707	7999.841245	12.023655	-0.058348	4.816019
287.303046	7999.869728	12.028659	-0.058366	4.816027
287.358033	7999.858965	12.033664	-0.058376	4.816024
287.365182	7999.938145	12.038669	-0.058377	4.816047
287.215266	7999.876657	12.043674	-0.058349	4.816030
287.153640	7999.852027	12.048679	-0.058338	4.816023
287.360740	7999.907055	12.053683	-0.058376	4.816038
287.058079	7999.878055	12.058688	-0.058320	4.816031
287.247084	7999.848353	12.063693	-0.058355	4.816021
287.262406	7999.950118	12.068698	-0.058358	4.816051
287.199938	7999.829319	12.073703	-0.058346	4.816016
287.256497	7999.870934	12.078707	-0.058356	4.816028
287.259398	7999.853883	12.083712	-0.058357	4.816023
287.371916	7999.858052	12.088717	-0.058378	4.816023
287.390295	7999.864786	12.093722	-0.058381	4.816025
287.138187	7999.943539	12.098727	-0.058334	4.816049
287.432476	7999.878354	12.103731	-0.058389	4.816029
287.198177	7999.831362	12.108736	-0.058345	4.816016
287.228704	7999.892804	12.113741	-0.058351	4.816034
287.483351	7999.858951	12.118746	-0.058398	4.816023
287.538203	7999.796903	12.123751	-0.058408	4.816005
287.437484	7999.818572	12.128755	-0.058389	4.816011
287.516307	7999.928967	12.133760	-0.058404	4.816043
287.411150	7999.834103	12.138765	-0.058384	4.816016
287.256246	7999.887909	12.143770	-0.058355	4.816033
287.245475	7999.832150	12.148775	-0.058353	4.816016
287.380751	7999.898696	12.153779	-0.058378	4.816035
287.319960	7999.867671	12.158784	-0.058367	4.816026
287.177417	7999.870419	12.163789	-0.058340	4.816028
287.516526	7999.904337	12.168794	-0.058403	4.816036
287.329074	7999.885972	12.173799	-0.058368	4.816032
287.069727	7999.981687	12.178803	-0.058320	4.816061
287.205381	7999.895464	12.183808	-0.058345	4.816035
287.354597	7999.841537	12.188813	-0.058373	4.816019
287.487130	7999.861025	12.193818	-0.058397	4.816024
287.290847	7999.948269	12.198823	-0.058361	4.816050
287.325490	7999.926452	12.203827	-0.058367	4.816044
287.040250	7999.912725	12.208832	-0.058314	4.816041
287.120520	7999.908830	12.213837	-0.058329	4.816040
287.312433	7999.894138	12.218842	-0.058364	4.816034
287.397318	7999.859344	12.223847	-0.058380	4.816024
287.478315	7999.887513	12.228851	-0.058395	4.816031
287.350322	7999.879842	12.233856	-0.058371	4.816030
287.395781	7999.941555	12.238861	-0.058380	4.816048
287.484782	7999.913245	12.243866	-0.058396	4.816039
287.439099	7999.899588	12.248871	-0.058387	4.816035
287.229639	7999.949199	12.253875	-0.058348	4.816051
287.307769	7999.928172	12.258880	-0.058363	4.816044
287.329591	7999.931764	12.263885	-0.058367	4.816045
287.401894	7999.913835	12.268890	-0.058380	4.816040
287.196834	7999.873784	12.273895	-0.058342	4.816029
287.295483	7999.918298	12.278899	-0.058360	4.816041
287.502763	7999.847262	12.283904	-0.058399	4.816020
287.452574	7999.841001	12.288909	-0.058389	4.816018
287.359306	7999.889515	12.293914	-0.058372	4.816033
287.412097	7999.915036	12.298919	-0.058381	4.816040
287.491937	7999.876945	12.303923	-0.058396	4.816028
287.404395	7999.861460	12.308928	-0.058380	4.816024
287.589261	7999.816727	12.313933	-0.058414	4.816010
287.703124	7999.930962	12.318938	-0.058435	4.816043
287.715062	7999.816854	12.323943	-0.058437	4.816010
287.677347	7999.839665	12.328947	-0.058430	4.816016
287.517731	7999.937189	12.333952	-0.058401	4.816046
287.735758	7999.819339	12.338957	-0.058441	4.816010
287.689765	7999.849480	12.343962	-0.058432	4.816019
287.303765	7999.895890	12.348967	-0.058360	4.816035
287.458475	7999.836721	12.353971	-0.058389	4.816017
287.390450	7999.851504	12.358976	-0.058376	4.816021
287.393478	7999.880397	12.363981	-0.058377	4.816030
287.448581	7999.903823	12.368986	-0.058387	4.816036
287.412415	7999.910637	12.373991	-0.058380	4.816039
287.428690	7999.822248	12.378995	-0.058383	4.816013
287.497105	7999.852326	12.384000	-0.058396	4.816021
287.526674	7999.880631	12.389005	-0.058401	4.816029
287.548447	7999.898111	12.394010	-0.058405	4.816034
287.636708	7999.856968	12.399015	-0.058421	4.816022
287.640798	7999.881606	12.404019	-0.058422	4.816029
287.636903	7999.897552	12.409024	-0.058421	4.816034
287.577515	7999.884715	12.414029	-0.058410	4.816030
287.829108	7999.899952	12.419034	-0.058457	4.816033
287.673620	7999.948406	12.424039	-0.058428	4.816048
287.731039	7999.856489	12.429043	-0.058438	4.816021
287.729666	7999.900259	12.434048	-0.058438	4.816034
287.603148	7999.905435	12.439053	-0.058415	4.816036
287.630831	7999.911270	12.444058	-0.058420	4.816038
287.453262	7999.861033	12.449063	-0.058386	4.816024
287.781930	7999.906514	12.454067	-0.058448	4.816035
287.753308	7999.891029	12.459072	-0.058442	4.816031
287.516299	7999.847192	12.464077	-0.058398	4.816020
287.613201	7999.926932	12.469082	-0.058416	4.816042
287.614710	7999.881010	12.474087	-0.058416	4.816029
287.711769	7999.893446	12.479091	-0.058434	4.816032
287.625163	7999.895071	12.484096	-0.058418	4.816033
287.726563	7999.887286	12.489101	-0.058437	4.816030
287.737015	7999.883193	12.494106	-0.058438	4.816029
287.598435	7999.883877	12.499111	-0.058413	4.816030
287.658916	7999.935179	12.504115	-0.058424	4.816045
287.630036	7999.866270	12.509120	-0.058418	4.816025
287.476067	7999.780136	12.514125	-0.058389	4.816000
287.489772	7999.887213	12.519130	-0.058392	4.816031
287.625943	7999.937751	12.524135	-0.058417	4.816045
287.536957	7999.848521	12.529139	-0.058401	4.816020
287.563524	7999.888524	12.534144	-0.058405	4.816031
287.497965	7999.834976	12.539149	-0.058393	4.816016
287.644753	7999.913484	12.544154	-0.058420	4.816038
287.532205	7999.879383	12.549159	-0.058399	4.816029
287.616031	7999.900125	12.554163	-0.058415	4.816035
287.670337	7999.889349	12.559168	-0.058425	4.816031
287.445427	7999.846800	12.564173	-0.058383	4.816020
287.461209	7999.936821	12.569178	-0.058386	4.816046
287.766980	7999.832314	12.574183	-0.058443	4.816014
287.947618	7999.872975	12.579187	-0.058476	4.816025
287.721777	7999.879554	12.584192	-0.058434	4.816028
287.696897	7999.805376	12.589197	-0.058429	4.816006
287.729936	7999.972634	12.594202	-0.058435	4.816055
287.486958	7999.807962	12.599207	-0.058390	4.816008
287.665848	7999.861411	12.604211	-0.058423	4.816023
287.666155	7999.926579	12.609216	-0.058423	4.816042
287.575728	7999.822366	12.614221	-0.058406	4.816012
287.733301	7999.865813	12.619226	-0.058435	4.816024
287.783700	7999.833598	12.624231	-0.058445	4.816014
287.750199	7999.917384	12.629235	-0.058438	4.816039
287.753653	7999.817010	12.634240	-0.058439	4.816010
287.734788	7999.910677	12.639245	-0.058435	4.816037
287.804336	7999.848895	12.644250	-0.058448	4.816019
287.589767	7999.898414	12.649255	-0.058408	4.816034
287.699662	7999.821338	12.654259	-0.058429	4.816011
287.625013	7999.879805	12.659264	-0.058415	4.816029
287.766681	7999.879160	12.664269	-0.058441	4.816028
287.722761	7999.840962	12.669274	-0.058433	4.816017
287.705651	7999.874831	12.674279	-0.058429	4.816027
287.664500	7999.838819	12.679283	-0.058422	4.816016
287.686797	7999.833873	12.684288	-0.058426	4.816015
287.657881	7999.955135	12.689293	-0.058420	4.816050
287.597141	7999.796973	12.694298	-0.058409	4.816005
287.595016	7999.928336	12.699303	-0.058408	4.816043
287.595847	7999.843941	12.704307	-0.058408	4.816018
287.739338	7999.868970	12.709312	-0.058435	4.816025
287.750853	7999.845666	12.714317	-0.058437	4.816018
287.914845	7999.889229	12.719322	-0.058467	4.816030
287.536932	7999.833222	12.724327	-0.058397	4.816015
287.862430	7999.886124	12.729331	-0.058458	4.816029
287.820598	7999.999674	12.734336	-0.058450	4.816063
287.862231	7999.829479	12.739341	-0.058457	4.816013
287.976457	7999.832610	12.744346	-0.058478	4.816013
287.702683	7999.851141	12.749351	-0.058427	4.816020
287.713499	7999.922910	12.754355	-0.058429	4.816041
287.805509	7999.873287	12.759360	-0.058446	4.816026
287.867124	7999.840208	12.764365	-0.058458	4.816016
287.816527	7999.913000	12.769370	-0.058448	4.816037
287.881742	7999.824430	12.774375	-0.058460	4.816011
287.901248	7999.853621	12.779379	-0.058464	4.816020
287.763229	7999.925896	12.784384	-0.058438	4.816041
287.656294	7999.889760	12.789389	-0.058418	4.816031
287.892764	7999.854509	12.794394	-0.058462	4.816020
287.771137	7999.854432	12.799399	-0.058439	4.816020
287.925129	7999.805933	12.804403	-0.058468	4.816005
287.962980	7999.960458	12.809408	-0.058475	4.816050
287.943044	7999.843634	12.814413	-0.058471	4.816016
287.853018	7999.886864	12.819418	-0.058454	4.816030
287.930096	7999.881843	12.824423	-0.058468	4.816028
287.917757	7999.817508	12.829427	-0.058466	4.816009
287.848112	7999.943374	12.834432	-0.058453	4.816046
287.750410	7999.829413	12.839437	-0.058435	4.816013
287.864171	7999.867792	12.844442	-0.058456	4.816024
287.911161	7999.873977	12.849447	-0.058464	4.816025
287.926310	7999.852876	12.854451	-0.058467	4.816019
287.929634	7999.864679	12.859456	-0.058468	4.816023
287.962859	7999.918692	12.864461	-0.058474	4.816038
287.965217	7999.847145	12.869466	-0.058474	4.816017
288.012547	7999.845858	12.874471	-0.058483	4.816017
288.051962	7999.912804	12.879475	-0.058490	4.816036
287.973484	7999.852610	12.884480	-0.058475	4.816019
287.887526	7999.901257	12.889485	-0.058459	4.816034
287.891579	7999.801962	12.894490	-0.058460	4.816005
287.837397	7999.925971	12.899495	-0.058450	4.816041
287.868683	7999.807940	12.904499	-0.058456	4.816006
288.116530	7999.845545	12.909504	-0.058502	4.816016
287.960911	7999.864082	12.914509	-0.058473	4.816022
287.880825	7999.896809	12.919514	-0.058458	4.816032
287.920052	7999.904990	12.924519	-0.058465	4.816035
287.911449	7999.881321	12.929523	-0.058463	4.816028
287.925749	7999.878367	12.934528	-0.058466	4.816027
287.787318	7999.873711	12.939533	-0.058440	4.816026
287.820978	7999.901022	12.944538	-0.058446	4.816034
287.742511	7999.860060	12.949543	-0.058431	4.816022
287.757073	7999.804760	12.954547	-0.058434	4.816006
287.868263	7999.866596	12.959552	-0.058454	4.816024
287.659147	7999.945061	12.964557	-0.058416	4.816048
287.843788	7999.859725	12.969562	-0.058450	4.816022
287.697525	7999.810055	12.974567	-0.058422	4.816008
287.855409	7999.906927	12.979571	-0.058452	4.816035
287.855360	7999.841746	12.984576	-0.058452	4.816016
287.994001	7999.882713	12.989581	-0.058477	4.816028
288.217829	7999.844028	12.994586	-0.058519	4.816015
287.973991	7999.820367	12.999591	-0.058473	4.816010
287.825501	7999.823007	13.004595	-0.058446	4.816011
287.803455	7999.957214	13.009600	-0.058442	4.816050
287.933896	7999.833502	13.014605	-0.058466	4.816014
288.084841	7999.869351	13.019610	-0.058494	4.816023
288.045221	7999.837640	13.024615	-0.058486	4.816014
287.998340	7999.904090	13.029619	-0.058477	4.816034
288.032138	7999.839522	13.034624	-0.058484	4.816015
287.877436	7999.895469	13.039629	-0.058455	4.816032
287.984618	7999.867489	13.044634	-0.058475	4.816023
287.913958	7999.849105	13.049639	-0.058461	4.816018
288.073039	7999.880828	13.054643	-0.058491	4.816027
288.094584	7999.866252	13.059648	-0.058495	4.816022
288.051150	7999.838746	13.064653	-0.058487	4.816015
288.193361	7999.892599	13.069658	-0.058513	4.816030
288.016048	7999.926768	13.074663	-0.058480	4.816040
288.070686	7999.858305	13.079667	-0.058490	4.816020
288.076813	7999.840245	13.084672	-0.058491	4.816015
287.883632	7999.886947	13.089677	-0.058455	4.816030
287.996970	7999.836643	13.094682	-0.058476	4.816014
287.835135	7999.924511	13.099687	-0.058446	4.816041
287.936968	7999.800280	13.104691	-0.058465	4.816004
288.061949	7999.866641	13.109696	-0.058488	4.816023
287.955123	7999.904225	13.114701	-0.058468	4.816034
288.146644	7999.829698	13.119706	-0.058503	4.816011
287.964873	7999.842418	13.124711	-0.058469	4.816016
287.921944	7999.917486	13.129715	-0.058461	4.816038
287.992907	7999.803379	13.134720	-0.058475	4.816005
287.900617	7999.939518	13.139725	-0.058457	4.816045
288.039598	7999.853354	13.144730	-0.058483	4.816019
288.095685	7999.805217	13.149735	-0.058493	4.816005
287.967890	7999.883019	13.154739	-0.058470	4.816028
287.899091	7999.834754	13.159744	-0.058457	4.816014
287.954430	7999.940450	13.164749	-0.058467	4.816045
288.034861	7999.845745	13.169754	-0.058482	4.816017
288.002059	7999.797065	13.174759	-0.058475	4.816003
287.830419	7999.894371	13.179763	-0.058444	4.816032
288.069640	7999.866649	13.184768	-0.058488	4.816023
288.026958	7999.826336	13.189773	-0.058480	4.816011
288.014829	7999.866706	13.194778	-0.058478	4.816023
288.030076	7999.892615	13.199783	-0.058480	4.816030
287.897008	7999.785492	13.204787	-0.058455	4.816000
287.948646	7999.900736	13.209792	-0.058465	4.816033
288.004628	7999.830161	13.214797	-0.058475	4.816012
288.087066	7999.835921	13.219802	-0.058491	4.816014
287.996830	7999.931499	13.224807	-0.058474	4.816042
287.952049	7999.839865	13.229811	-0.058465	4.816015
288.296217	7999.887765	13.234816	-0.058529	4.816028
288.016133	7999.822847	13.239821	-0.058477	4.816010
288.117260	7999.848177	13.244826	-0.058496	4.816017
288.181768	7999.946561	13.249831	-0.058508	4.816045
288.215734	7999.804005	13.254835	-0.058514	4.816004
288.006816	7999.855763	13.259840	-0.058475	4.816020
288.014889	7999.895431	13.264845	-0.058476	4.816031
288.253383	7999.820687	13.269850	-0.058521	4.816008
288.157231	7999.952483	13.274855	-0.058503	4.816047
288.090938	7999.883963	13.279859	-0.058490	4.816028
288.174087	7999.881189	13.284864	-0.058506	4.816026
288.031813	7999.859369	13.289869	-0.058479	4.816021
288.176288	7999.880143	13.294874	-0.058506	4.816026
288.179334	7999.896215	13.299879	-0.058506	4.816031
288.088859	7999.858240	13.304883	-0.058489	4.816020
288.248022	7999.888896	13.309888	-0.058519	4.816028
288.161364	7999.800777	13.314893	-0.058503	4.816003
288.316594	7999.862345	13.319898	-0.058531	4.816020
288.231620	7999.959087	13.324903	-0.058516	4.816049
288.064025	7999.791507	13.329907	-0.058484	4.816001
288.070657	7999.920893	13.334912	-0.058485	4.816039
288.031804	7999.782358	13.339917	-0.058478	4.815998
287.966799	7999.952111	13.344922	-0.058466	4.816048
287.950561	7999.826807	13.349927	-0.058463	4.816012
288.068779	7999.826806	13.354931	-0.058485	4.816011
288.005503	7999.899368	13.359936	-0.058473	4.816033
287.934428	7999.842514	13.364941	-0.058460	4.816016
288.153949	7999.941573	13.369946	-0.058500	4.816044
288.218210	7999.886105	13.374951	-0.058512	4.816028
288.174196	7999.859657	13.379955	-0.058504	4.816020
288.113394	7999.891665	13.384960	-0.058493	4.816030
288.218263	7999.865780	13.389965	-0.058512	4.816022
288.294855	7999.879981	13.394970	-0.058526	4.816025
288.065170	7999.817046	13.399975	-0.058483	4.816008
288.143910	7999.913551	13.404979	-0.058498	4.816036
288.022956	7999.855793	13.409984	-0.058475	4.816020
287.970967	7999.824927	13.414989	-0.058465	4.816011
288.074351	7999.841750	13.419994	-0.058485	4.816015
288.032668	7999.837780	13.424999	-0.058477	4.816015
288.079834	7999.920893	13.430003	-0.058485	4.816039
288.167776	7999.895769	13.435008	-0.058502	4.816031
288.054506	7999.806099	13.440013	-0.058480	4.816005
288.240113	7999.901337	13.445018	-0.058515	4.816032
288.191628	7999.969895	13.450023	-0.058506	4.816052
288.231106	7999.861626	13.455027	-0.058513	4.816020
288.352430	7999.872365	13.460032	-0.058536	4.816023
288.162276	7999.862497	13.465037	-0.058500	4.816021
288.371880	7999.875905	13.470042	-0.058539	4.816024
288.250552	7999.872627	13.475047	-0.058516	4.816024
288.226324	7999.807008	13.480051	-0.058512	4.816005
288.401300	7999.900986	13.485056	-0.058544	4.816031
288.067479	7999.889580	13.490061	-0.058482	4.816030
288.267832	7999.873974	13.495066	-0.058519	4.816024
288.273460	7999.885820	13.500071	-0.058520	4.816027
288.369344	7999.867251	13.505075	-0.058538	4.816021
288.261396	7999.903746	13.510080	-0.058518	4.816033
288.044102	7999.855992	13.515085	-0.058477	4.816020
288.177739	7999.851997	13.520090	-0.058502	4.816018
287.908052	7999.967825	13.525095	-0.058452	4.816053
287.900294	7999.814897	13.530099	-0.058450	4.816009
288.058133	7999.857280	13.535104	-0.058479	4.816020
288.078192	7999.818105	13.540109	-0.058483	4.816009
288.308577	7999.889583	13.545114	-0.058526	4.816028
288.089555	7999.879192	13.550119	-0.058485	4.816026
288.011983	7999.859613	13.555123	-0.058471	4.816021
288.302976	7999.875566	13.560128	-0.058525	4.816024
288.031574	7999.830036	13.565133	-0.058474	4.816012
288.157678	7999.860093	13.570138	-0.058497	4.816020
288.506034	7999.864265	13.575143	-0.058562	4.816020
288.225565	7999.849554	13.580147	-0.058510	4.816017
288.001906	7999.876472	13.585152	-0.058468	4.816026
287.890993	7999.906503	13.590157	-0.058447	4.816035
288.071039	7999.824289	13.595162	-0.058481	4.816010
287.853622	7999.856663	13.600167	-0.058440	4.816021
288.091709	7999.846014	13.605171	-0.058484	4.816017
288.307630	7999.880905	13.610176	-0.058525	4.816026
288.245140	7999.931045	13.615181	-0.058513	4.816041
288.310699	7999.863849	13.620186	-0.058525	4.816021
288.186456	7999.832740	13.625191	-0.058502	4.816012
288.159073	7999.807662	13.630195	-0.058497	4.816005
288.178818	7999.903098	13.635200	-0.058500	4.816033
288.113128	7999.901898	13.640205	-0.058488	4.816033
288.278568	7999.816213	13.645210	-0.058519	4.816007
288.011703	7999.859442	13.650215	-0.058469	4.816021
288.157457	7999.866350	13.655219	-0.058496	4.816022
288.214506	7999.857760	13.660224	-0.058506	4.816020
288.058715	7999.820738	13.665229	-0.058477	4.816010
288.134282	7999.880861	13.670234	-0.058491	4.816027
287.929888	7999.882487	13.675239	-0.058453	4.816028
287.958499	7999.930006	13.680243	-0.058458	4.816042
288.051190	7999.880396	13.685248	-0.058476	4.816027
288.046699	7999.871759	13.690253	-0.058475	4.816025
288.206473	7999.862895	13.695258	-0.058504	4.816021
288.119029	7999.857027	13.700263	-0.058488	4.816020
288.013786	7999.809169	13.705267	-0.058468	4.816006
288.221919	7999.958236	13.710272	-0.058507	4.816049
288.149126	7999.845794	13.715277	-0.058493	4.816016
288.058905	7999.884748	13.720282	-0.058476	4.816028
288.186255	7999.888117	13.725287	-0.058500	4.816029
288.228693	7999.824775	13.730291	-0.058508	4.816010
288.196767	7999.840213	13.735296	-0.058502	4.816015
288.135161	7999.922421	13.740301	-0.058490	4.816039
288.133709	7999.898882	13.745306	-0.058490	4.816032
288.333152	7999.925995	13.750311	-0.058527	4.816039
288.194912	7999.836939	13.755315	-0.058501	4.816014
288.200406	7999.849851	13.760320	-0.058502	4.816017
288.045928	7999.871613	13.765325	-0.058473	4.816025
288.001286	7999.852632	13.770330	-0.058465	4.816019
288.269435	7999.950437	13.775335	-0.058515	4.816046
288.215335	7999.819103	13.780339	-0.058504	4.816008
288.188330	7999.865614	13.785344	-0.058499	4.816022
288.125833	7999.873019	13.790349	-0.058488	4.816025
288.217540	7999.872536	13.795354	-0.058505	4.816024
288.192178	7999.853905	13.800359	-0.058500	4.816019
288.149441	7999.919361	13.805363	-0.058492	4.816038
288.254459	7999.865701	13.810368	-0.058511	4.816022
288.072468	7999.866665	13.815373	-0.058477	4.816023
288.189616	7999.843140	13.820378	-0.058499	4.816015
288.160695	7999.875726	13.825383	-0.058493	4.816025
288.175807	7999.917659	13.830387	-0.058496	4.816037
288.141183	7999.895654	13.835392	-0.058490	4.816031
288.132152	7999.836721	13.840397	-0.058488	4.816014
288.310574	7999.859179	13.845402	-0.058521	4.816020
288.252919	7999.852782	13.850407	-0.058510	4.816018
288.123632	7999.863249	13.855411	-0.058486	4.816022
288.245649	7999.893232	13.860416	-0.058509	4.816030
288.157699	7999.949321	13.865421	-0.058492	4.816047
288.111458	7999.855524	13.870426	-0.058483	4.816020
288.411036	7999.851333	13.875431	-0.058539	4.816017
288.300157	7999.819398	13.880435	-0.058518	4.816008
288.491056	7999.862382	13.885440	-0.058554	4.816020
288.309948	7999.925329	13.890445	-0.058520	4.816039
288.266039	7999.898882	13.895450	-0.058512	4.816031
288.199645	7999.881643	13.900455	-0.058499	4.816027
288.321834	7999.892398	13.905459	-0.058522	4.816029
288.401499	7999.934433	13.910464	-0.058537	4.816041
288.122583	7999.865262	13.915469	-0.058485	4.816022
288.177540	7999.855566	13.920474	-0.058495	4.816019
288.250468	7999.846196	13.925479	-0.058508	4.816016
288.248054	7999.910247	13.930483	-0.058508	4.816035
288.417652	7999.901562	13.935488	-0.058539	4.816031
288.127449	7999.816161	13.940493	-0.058485	4.816008
288.347711	7999.845788	13.945498	-0.058526	4.816015
288.478653	7999.878069	13.950503	-0.058550	4.816024
288.375136	7999.921055	13.955507	-0.058531	4.816037
288.401239	7999.899084	13.960512	-0.058536	4.816031
288.271850	7999.818736	13.965517	-0.058512	4.816008
288.131657	7999.838621	13.970522	-0.058485	4.816015
288.379133	7999.839895	13.975527	-0.058531	4.816014
288.506000	7999.906291	13.980531	-0.058555	4.816032
288.379347	7999.897575	13.985536	-0.058531	4.816030
288.182004	7999.815994	13.990541	-0.058494	4.816008
288.274535	7999.872151	13.995546	-0.058512	4.816024
288.301375	7999.826689	14.000551	-0.058516	4.816010
288.160377	7999.874337	14.005555	-0.058490	4.816025
288.424028	7999.872700	14.010560	-0.058539	4.816023
288.110604	7999.834955	14.015565	-0.058481	4.816014
288.284992	7999.909691	14.020570	-0.058513	4.816035
288.253163	7999.859959	14.025575	-0.058507	4.816020
288.257209	7999.800194	14.030579	-0.058508	4.816003
287.985007	7999.871104	14.035584	-0.058457	4.816025
288.165094	7999.836968	14.040589	-0.058490	4.816014
288.442181	7999.859079	14.045594	-0.058542	4.816019
288.337293	7999.986443	14.050599	-0.058522	4.816057
288.116620	7999.826447	14.055603	-0.058481	4.816011
288.114895	7999.873416	14.060608	-0.058481	4.816025
288.142907	7999.845069	14.065613	-0.058486	4.816016
288.341762	7999.808068	14.070618	-0.058523	4.816005
288.279288	7999.988552	14.075623	-0.058511	4.816058
288.207973	7999.843017	14.080627	-0.058498	4.816015
288.317838	7999.864232	14.085632	-0.058518	4.816021
288.202622	7999.843971	14.090637	-0.058496	4.816016
288.269970	7999.856936	14.095642	-0.058509	4.816019
288.209954	7999.911395	14.100647	-0.058498	4.816035
288.177754	7999.862725	14.105651	-0.058492	4.816021
288.326072	7999.878227	14.110656	-0.058519	4.816025
288.269451	7999.935952	14.115661	-0.058508	4.816042
288.407365	7999.907462	14.120666	-0.058534	4.816033
288.364388	7999.876758	14.125671	-0.058526	4.816025
288.394301	7999.829215	14.130675	-0.058531	4.816010
288.565339	7999.902822	14.135680	-0.058563	4.816031
288.278026	7999.942474	14.140685	-0.058510	4.816044
288.434352	7999.863035	14.145690	-0.058539	4.816020
288.369183	7999.870391	14.150695	-0.058526	4.816023
288.253278	7999.904606	14.155699	-0.058505	4.816033
288.357324	7999.941741	14.160704	-0.058524	4.816044
288.281915	7999.873056	14.165709	-0.058510	4.816024
288.343941	7999.909429	14.170714	-0.058521	4.816034
288.257313	7999.857635	14.175719	-0.058505	4.816020
288.185089	7999.904393	14.180723	-0.058492	4.816034
288.179958	7999.869035	14.185728	-0.058490	4.816023
288.164880	7999.868753	14.190733	-0.058488	4.816023
288.240162	7999.838058	14.195738	-0.058502	4.816014
288.392246	7999.885679	14.200743	-0.058530	4.816027
288.363261	7999.846683	14.205747	-0.058524	4.816016
288.311276	7999.867099	14.210752	-0.058514	4.816022
288.239737	7999.890366	14.215757	-0.058501	4.816029
288.238655	7999.888201	14.220762	-0.058501	4.816029
288.134576	7999.867073	14.225767	-0.058481	4.816023
288.062757	7999.918113	14.230771	-0.058468	4.816038
288.304679	7999.844499	14.235776	-0.058513	4.816015
288.188864	7999.823159	14.240781	-0.058491	4.816010
288.132156	7999.883020	14.245786	-0.058481	4.816028
288.251284	7999.877693	14.250791	-0.058503	4.816025
288.252863	7999.863824	14.255795	-0.058503	4.816021
288.476388	7999.620004	14.260800	-0.058544	4.815949

288.457212	7996.351809	14.265805	-0.058538	4.814994
288.362228	7990.782702	14.270810	-0.058517	4.813366
288.300751	7984.038766	14.275815	-0.058501	4.811395
288.254716	7976.663087	14.280819	-0.058488	4.809237
288.210077	7969.067891	14.285824	-0.058474	4.807014
287.962753	7961.184961	14.290829	-0.058423	4.804707
287.890673	7953.376015	14.295834	-0.058404	4.802419
288.074430	7945.391974	14.300839	-0.058433	4.800078
287.835179	7937.470727	14.305843	-0.058383	4.797756
287.854025	7929.447017	14.310848	-0.058382	4.795402
287.904040	7921.433072	14.315853	-0.058386	4.793049
287.662622	7913.374809	14.320858	-0.058335	4.790684
287.878024	7905.413898	14.325863	-0.058370	4.788344
287.762783	7897.346528	14.330867	-0.058343	4.785972
287.883634	7889.438602	14.335872	-0.058361	4.783646
287.855393	7881.454785	14.340877	-0.058350	4.781297
287.610911	7873.426072	14.345882	-0.058299	4.778934
287.617611	7865.422117	14.350887	-0.058295	4.776576
287.516687	7857.403598	14.355891	-0.058271	4.774213
287.670559	7849.394898	14.360896	-0.058294	4.771851
287.472480	7841.379802	14.365901	-0.058252	4.769488
287.432483	7833.416461	14.370906	-0.058240	4.767137
287.434358	7825.368867	14.375911	-0.058235	4.764761
287.312522	7817.456715	14.380915	-0.058207	4.762424
287.273673	7809.404961	14.385920	-0.058194	4.760044
287.413409	7801.415567	14.390925	-0.058215	4.757681
287.131723	7793.387660	14.395930	-0.058157	4.755306
287.234760	7785.359352	14.400935	-0.058171	4.752929
287.174959	7777.290811	14.405939	-0.058154	4.750540
287.263219	7769.315633	14.410944	-0.058165	4.748176
286.984387	7761.303037	14.415949	-0.058108	4.745801
287.003970	7753.263460	14.420954	-0.058107	4.743416
287.228044	7745.399687	14.425959	-0.058143	4.741082
287.073159	7737.356567	14.430963	-0.058109	4.738694
287.111355	7729.366025	14.435968	-0.058111	4.736320
286.777354	7721.352161	14.440973	-0.058043	4.733939
286.965460	7713.315747	14.445978	-0.058073	4.731549
286.813900	7705.347800	14.450983	-0.058039	4.729179
286.745722	7697.307222	14.455987	-0.058021	4.726785
286.666861	7689.325133	14.460992	-0.058001	4.724408
286.531763	7681.369562	14.465997	-0.057971	4.722038
286.671515	7673.285789	14.471002	-0.057992	4.719627
286.617696	7665.401936	14.476007	-0.057976	4.717276
286.601569	7657.347754	14.481011	-0.057968	4.714872
286.658831	7649.314078	14.486016	-0.057973	4.712473
286.564362	7641.247533	14.491021	-0.057950	4.710064
286.366711	7633.334585	14.496026	-0.057908	4.707699
286.384811	7625.284648	14.501031	-0.057906	4.705292
286.443640	7617.319516	14.506035	-0.057912	4.702908
286.298268	7609.350395	14.511040	-0.057880	4.700523
286.059594	7601.324158	14.516045	-0.057830	4.698120
286.134804	7593.304706	14.521050	-0.057839	4.695717
286.093071	7585.350864	14.526055	-0.057826	4.693332
286.009269	7577.208268	14.531059	-0.057805	4.690890
286.065224	7569.256132	14.536064	-0.057810	4.688503
285.757901	7561.277270	14.541069	-0.057747	4.686108
285.916118	7553.292475	14.546074	-0.057771	4.683708
286.152178	7545.335111	14.551079	-0.057810	4.681316
285.984617	7537.290756	14.556083	-0.057774	4.678897
285.891534	7529.367307	14.561088	-0.057751	4.676513
285.684599	7521.239857	14.566093	-0.057707	4.674067
285.594718	7513.135099	14.571098	-0.057685	4.671626
285.678392	7505.220021	14.576103	-0.057695	4.669240
285.259171	7497.220101	14.581107	-0.057612	4.666829
285.419450	7489.229838	14.586112	-0.057637	4.664418
285.379630	7481.298398	14.591117	-0.057624	4.662024
285.437617	7473.237214	14.596122	-0.057629	4.659589
285.468931	7465.304052	14.601127	-0.057630	4.657192
285.253813	7457.216835	14.606131	-0.057584	4.654748
285.233489	7449.239095	14.611136	-0.057575	4.652335
285.048062	7441.171946	14.616141	-0.057535	4.649894
285.059961	7433.224382	14.621146	-0.057532	4.647487
285.243128	7425.221886	14.626151	-0.057561	4.645063
284.992594	7417.268149	14.631155	-0.057509	4.642652
285.073591	7409.204608	14.636160	-0.057519	4.640207
285.011076	7401.252801	14.641165	-0.057502	4.637794
284.978805	7393.223015	14.646170	-0.057491	4.635356
284.903512	7385.276463	14.651175	-0.057472	4.632943
284.891666	7377.189464	14.656179	-0.057464	4.630485
284.955034	7369.177806	14.661184	-0.057470	4.628049
284.778149	7361.162558	14.666189	-0.057432	4.625611
284.959208	7353.223207	14.671194	-0.057461	4.623194
284.978530	7345.220981	14.676199	-0.057459	4.620757
284.680838	7337.215188	14.681203	-0.057398	4.618318
284.679536	7329.191747	14.686208	-0.057393	4.615872
284.762223	7321.147119	14.691213	-0.057403	4.613418
284.527217	7313.143131	14.696218	-0.057354	4.610975
284.409186	7305.214149	14.701223	-0.057326	4.608554
284.414543	7297.182241	14.706227	-0.057322	4.606100
284.456008	7289.178132	14.711232	-0.057324	4.603653
284.386845	7281.194534	14.716237	-0.057306	4.601212
284.531427	7273.175514	14.721242	-0.057328	4.598758
284.329410	7265.185125	14.726247	-0.057285	4.596311
284.095467	7257.131833	14.731251	-0.057236	4.593844
284.131443	7249.131794	14.736256	-0.057238	4.591392
284.429214	7241.125742	14.741261	-0.057288	4.588937
284.327479	7233.106809	14.746266	-0.057263	4.586477
283.940742	7225.174802	14.751271	-0.057186	4.584042
284.147651	7217.148023	14.756275	-0.057219	4.581576
284.039817	7209.194923	14.761280	-0.057194	4.579132
283.829680	7201.174191	14.766285	-0.057150	4.576666
283.826727	7193.158564	14.771290	-0.057144	4.574199
283.920761	7185.127834	14.776295	-0.057156	4.571727
283.673929	7177.119314	14.781299	-0.057105	4.569261
283.626365	7169.184682	14.786304	-0.057090	4.566816
283.659193	7161.118490	14.791309	-0.057091	4.564329
283.765821	7153.164759	14.796314	-0.057106	4.561875
283.497782	7145.137426	14.801319	-0.057051	4.559397
283.433604	7137.181686	14.806323	-0.057033	4.556940
283.509026	7129.154077	14.811328	-0.057042	4.554460
283.356824	7121.115424	14.816333	-0.057008	4.551974
283.272710	7113.076954	14.821338	-0.056987	4.549488
283.467505	7105.142729	14.826343	-0.057018	4.547032
283.260838	7097.081250	14.831347	-0.056975	4.544535
283.357084	7089.151986	14.836352	-0.056987	4.542079
283.248833	7081.116109	14.841357	-0.056962	4.539587
283.225348	7073.150724	14.846362	-0.056952	4.537117
283.067698	7065.134008	14.851367	-0.056917	4.534628
282.955122	7057.113501	14.856371	-0.056891	4.532138
283.151122	7049.074792	14.861376	-0.056922	4.529640
283.103179	7041.166234	14.866381	-0.056908	4.527182
283.129649	7033.074946	14.871386	-0.056908	4.524665
283.036642	7025.152310	14.876391	-0.056885	4.522199
282.890034	7017.102043	14.881395	-0.056853	4.519692
283.035792	7009.143698	14.886400	-0.056874	4.517213
282.874726	7001.137524	14.891405	-0.056839	4.514717
282.811103	6993.008135	14.896410	-0.056822	4.512182
282.591659	6985.056406	14.901415	-0.056776	4.509700
282.480704	6977.074421	14.906419	-0.056750	4.507207
282.510197	6969.062949	14.911424	-0.056750	4.504704
282.514409	6961.111025	14.916429	-0.056745	4.502218
282.348794	6953.056987	14.921434	-0.056709	4.499699
282.396876	6945.123591	14.926439	-0.056713	4.497216
282.426935	6937.055156	14.931443	-0.056713	4.494690
282.368680	6929.053728	14.936448	-0.056697	4.492183
282.456889	6921.055595	14.941453	-0.056708	4.489676
282.395807	6913.091022	14.946458	-0.056692	4.487178
282.175264	6905.071620	14.951463	-0.056645	4.484660
282.091489	6897.093385	14.956467	-0.056624	4.482155
282.213275	6889.083035	14.961472	-0.056642	4.479639
282.091752	6881.111153	14.966477	-0.056614	4.477132
281.948425	6873.036827	14.971482	-0.056582	4.474592
281.963967	6865.029101	14.976487	-0.056579	4.472072
281.951267	6856.991476	14.981491	-0.056572	4.469541
282.051174	6849.026638	14.986496	-0.056585	4.467032
281.875861	6841.026469	14.991501	-0.056547	4.464509
281.825044	6833.063253	14.996506	-0.056532	4.461998
281.867263	6825.090711	15.001511	-0.056535	4.459481
281.817363	6817.037662	15.006515	-0.056520	4.456938
281.803423	6809.055028	15.011520	-0.056512	4.454416
281.635688	6801.015458	15.016525	-0.056476	4.451874
281.651416	6792.969597	15.021530	-0.056473	4.449329
281.758411	6785.008150	15.026535	-0.056488	4.446809
281.691134	6777.024644	15.031539	-0.056470	4.444281
281.525565	6769.054767	15.036544	-0.056434	4.441755
281.595631	6761.030532	15.041549	-0.056442	4.439211
281.603020	6753.024438	15.046554	-0.056438	4.436671
281.343188	6745.040042	15.051559	-0.056384	4.434136
281.210250	6736.961424	15.056563	-0.056354	4.431570
281.226076	6728.984825	15.061568	-0.056352	4.429035
281.063728	6721.000404	15.066573	-0.056316	4.426495
281.175751	6712.979713	15.071578	-0.056332	4.423944
281.134399	6705.006859	15.076583	-0.056319	4.421406
281.040317	6696.979557	15.081587	-0.056296	4.418849
280.886607	6689.027307	15.086592	-0.056262	4.416314
280.958610	6680.988429	15.091597	-0.056270	4.413750
280.895207	6672.961023	15.096602	-0.056253	4.411189
280.823201	6665.018602	15.101607	-0.056234	4.408653
280.728580	6656.965828	15.106611	-0.056211	4.406080
280.725022	6649.003357	15.111616	-0.056205	4.403535
280.870577	6640.990557	15.116621	-0.056227	4.400973
280.578332	6632.992948	15.121626	-0.056167	4.398412
280.704687	6625.009255	15.126631	-0.056186	4.395857
280.705012	6616.962965	15.131635	-0.056180	4.393279
280.658020	6608.992256	15.136640	-0.056166	4.390723
280.604061	6601.005892	15.141645	-0.056151	4.388162
280.610328	6592.961005	15.146650	-0.056147	4.385580
280.421761	6585.034859	15.151655	-0.056107	4.383033
280.329540	6576.992326	15.156659	-0.056084	4.380449
280.425706	6569.026169	15.161664	-0.056097	4.377888
280.434082	6560.992400	15.166669	-0.056093	4.375304
280.401427	6552.982511	15.171674	-0.056081	4.372725
280.308624	6544.963879	15.176679	-0.056059	4.370142
280.123642	6536.994267	15.181683	-0.056019	4.367573
280.199920	6528.984129	15.186688	-0.056028	4.364990
280.154602	6521.021524	15.191693	-0.056014	4.362421
280.130567	6512.958841	15.196698	-0.056005	4.359817
280.163173	6505.045842	15.201703	-0.056005	4.357261
279.858475	6497.013387	15.206707	-0.055943	4.354663
280.046608	6488.886865	15.211712	-0.055973	4.352036
280.024810	6480.948547	15.216717	-0.055964	4.349467
279.671772	6472.947062	15.221722	-0.055893	4.346874
279.654629	6464.966159	15.226727	-0.055884	4.344288
279.656149	6456.967516	15.231731	-0.055879	4.341695
279.628109	6448.971357	15.236736	-0.055869	4.339101
279.451284	6441.013734	15.241741	-0.055830	4.336517
279.509358	6432.905334	15.246746	-0.055836	4.333884
279.625657	6424.950483	15.251751	-0.055852	4.331299
279.415244	6416.948496	15.256755	-0.055808	4.328696
279.543205	6408.970307	15.261760	-0.055826	4.326101
279.466131	6400.963761	15.266765	-0.055807	4.323494
279.255995	6392.972556	15.271770	-0.055762	4.320889
279.337716	6385.031752	15.276775	-0.055772	4.318301
279.191163	6376.973319	15.281779	-0.055739	4.315672
279.227877	6368.957012	15.286784	-0.055741	4.313056
279.289134	6360.926866	15.291789	-0.055747	4.310434
279.015429	6352.961519	15.296794	-0.055691	4.307829
279.135935	6344.927415	15.301799	-0.055708	4.305203
279.174725	6336.946755	15.306803	-0.055710	4.302593
279.043450	6328.931882	15.311808	-0.055680	4.299968
279.043693	6320.983750	15.316813	-0.055675	4.297365
278.771271	6312.936267	15.321818	-0.055619	4.294725
278.998235	6304.943146	15.326823	-0.055656	4.292105
278.767493	6296.903733	15.331827	-0.055607	4.289465
278.731303	6288.945563	15.336832	-0.055595	4.286852
278.600110	6280.914740	15.341837	-0.055566	4.284212
278.619599	6272.931825	15.346842	-0.055564	4.281588
278.741392	6264.949427	15.351847	-0.055581	4.278963
278.652169	6256.948596	15.356851	-0.055560	4.276329
278.467183	6248.904876	15.361856	-0.055520	4.273678
278.480875	6240.879293	15.366861	-0.055517	4.271033
278.407310	6232.903453	15.371866	-0.055498	4.268402
278.430755	6224.913100	15.376871	-0.055497	4.265765
278.325626	6216.935676	15.381875	-0.055472	4.263130
278.446613	6208.898882	15.386880	-0.055489	4.260476
278.224931	6200.950471	15.391885	-0.055443	4.257846
278.163986	6192.879300	15.396890	-0.055426	4.255176
278.324522	6184.913030	15.401895	-0.055451	4.252540
278.206247	6176.866653	15.406899	-0.055423	4.249874
278.123418	6168.925200	15.411904	-0.055403	4.247241
278.165996	6160.917597	15.416909	-0.055405	4.244586
278.171524	6152.956436	15.421914	-0.055401	4.241944
277.905694	6144.941815	15.426919	-0.055346	4.239280
277.954593	6136.954737	15.431923	-0.055350	4.236627
277.916497	6128.927173	15.436928	-0.055338	4.233958
277.973598	6120.939579	15.441933	-0.055343	4.231301
277.653182	6112.884093	15.446938	-0.055278	4.228616
277.817282	6104.910176	15.451943	-0.055303	4.225962
277.680924	6096.955341	15.456947	-0.055273	4.223309
277.613506	6088.952134	15.461952	-0.055255	4.220639
277.750290	6080.967801	15.466957	-0.055275	4.217976
277.696573	6072.920140	15.471962	-0.055260	4.215287
277.614435	6064.915829	15.476967	-0.055239	4.212612
277.472781	6056.932389	15.481971	-0.055207	4.209941
277.617757	6048.927904	15.486976	-0.055229	4.207264
277.270146	6040.955207	15.491981	-0.055159	4.204591
277.173176	6032.974648	15.496986	-0.055136	4.201917
277.285757	6024.996638	15.501991	-0.055151	4.199244
277.108948	6016.974748	15.506995	-0.055113	4.196551
277.248475	6008.895448	15.512000	-0.055134	4.193840
277.330918	6000.823074	15.517005	-0.055144	4.191130
277.231845	5992.821857	15.522010	-0.055120	4.188440
277.025053	5984.878360	15.527015	-0.055076	4.185766
277.027459	5976.933491	15.532019	-0.055071	4.183092
277.015027	5968.886666	15.537024	-0.055064	4.180382
277.100322	5960.972574	15.542029	-0.055074	4.177716
276.881002	5952.888085	15.547034	-0.055028	4.174988
277.206566	5944.905296	15.552039	-0.055083	4.172298
276.936150	5936.906065	15.557043	-0.055028	4.169594
276.712446	5928.929104	15.562048	-0.054981	4.166897
276.877471	5920.922569	15.567053	-0.055006	4.164192
276.755720	5912.903833	15.572058	-0.054978	4.161478
276.735845	5904.910073	15.577063	-0.054969	4.158772
276.555233	5896.926870	15.582067	-0.054930	4.156066
276.573336	5888.935865	15.587072	-0.054928	4.153358
276.492404	5880.923954	15.592077	-0.054908	4.150639
276.183492	5872.882739	15.597082	-0.054845	4.147907
276.323260	5864.876735	15.602087	-0.054866	4.145189
276.259688	5856.904924	15.607091	-0.054849	4.142479
276.151464	5848.891258	15.612096	-0.054823	4.139753
276.082697	5840.974191	15.617101	-0.054805	4.137058
276.048931	5832.907122	15.622106	-0.054794	4.134311
276.178400	5824.887357	15.627111	-0.054812	4.131579
276.127503	5816.864547	15.632115	-0.054798	4.128843
276.097503	5808.889337	15.637120	-0.054787	4.126122
276.028574	5800.943646	15.642125	-0.054769	4.123408
276.047823	5792.909631	15.647130	-0.054767	4.120664
275.849328	5784.968219	15.652135	-0.054725	4.117946
275.785548	5776.928741	15.657139	-0.054708	4.115195
275.606211	5768.887933	15.662144	-0.054669	4.112440
275.651680	5760.848027	15.667149	-0.054672	4.109687
275.652754	5752.857010	15.672154	-0.054667	4.106947
275.658925	5744.899348	15.677159	-0.054663	4.104218
275.649501	5736.921197	15.682163	-0.054656	4.101479
275.502776	5728.934427	15.687168	-0.054623	4.098734
275.361392	5720.941073	15.692173	-0.054591	4.095985
275.293019	5712.918639	15.697178	-0.054573	4.093225
275.364761	5704.887276	15.702183	-0.054581	4.090461
275.320029	5696.892033	15.707187	-0.054568	4.087707
275.221048	5688.909716	15.712192	-0.054544	4.084955
275.260899	5680.970017	15.717197	-0.054546	4.082217
275.272364	5672.892040	15.722202	-0.054543	4.079429
275.408385	5664.983741	15.727207	-0.054563	4.076700
275.154683	5656.917097	15.732211	-0.054510	4.073909
275.186363	5648.924310	15.737216	-0.054511	4.071146
275.099493	5640.939819	15.742221	-0.054490	4.068381
274.912063	5632.913414	15.747226	-0.054449	4.065599
274.989343	5624.961296	15.752231	-0.054459	4.062845
275.026320	5616.907258	15.757235	-0.054460	4.060052
274.904090	5608.973088	15.762240	-0.054432	4.057298
274.618057	5601.004250	15.767245	-0.054374	4.054526
274.754447	5592.945684	15.772250	-0.054394	4.051728
274.612569	5584.958747	15.777255	-0.054362	4.048949
274.409415	5576.941307	15.782259	-0.054319	4.046156
274.663691	5568.936633	15.787264	-0.054361	4.043373
274.579538	5560.969301	15.792269	-0.054340	4.040595
274.416348	5552.956180	15.797274	-0.054304	4.037799
274.493990	5544.952929	15.802279	-0.054313	4.035008
274.545632	5536.788245	15.807283	-0.054317	4.032158
274.319167	5528.836663	15.812288	-0.054270	4.029376
274.297897	5520.897150	15.817293	-0.054261	4.026600
274.247035	5512.901952	15.822298	-0.054246	4.023801
274.151873	5504.943654	15.827303	-0.054223	4.021013
274.024095	5496.947789	15.832307	-0.054194	4.018210
273.962845	5488.926211	15.837312	-0.054177	4.015396
274.064649	5480.898771	15.842317	-0.054191	4.012581
273.800541	5472.863536	15.847322	-0.054136	4.009756
273.846172	5464.949321	15.852327	-0.054140	4.006976
273.820460	5456.916797	15.857331	-0.054129	4.004151
273.756491	5448.938657	15.862336	-0.054112	4.001343
273.824395	5440.940807	15.867341	-0.054120	3.998527
273.664168	5432.926842	15.872346	-0.054084	3.995701
273.776997	5424.930305	15.877351	-0.054100	3.992883
273.677388	5416.872855	15.882355	-0.054076	3.990038
273.666302	5408.905588	15.887360	-0.054069	3.987225
273.692927	5400.927233	15.892365	-0.054069	3.984406
273.631629	5392.949697	15.897370	-0.054052	3.981584
273.634323	5384.929946	15.902375	-0.054047	3.978746
273.535677	5376.941727	15.907379	-0.054023	3.975916
273.462348	5368.913163	15.912384	-0.054004	3.973069
273.461305	5360.913446	15.917389	-0.053999	3.970232
273.196421	5352.950188	15.922394	-0.053944	3.967402
273.345788	5344.948788	15.927399	-0.053967	3.964563
273.154099	5336.986615	15.932403	-0.053926	3.961730
272.926541	5329.002956	15.937408	-0.053878	3.958887
272.989249	5321.000016	15.942413	-0.053885	3.956039
272.873751	5312.961331	15.947418	-0.053858	3.953174
272.819758	5304.977260	15.952423	-0.053842	3.950328
272.865798	5296.960938	15.957427	-0.053846	3.947469
272.791741	5288.953558	15.962432	-0.053827	3.944610
272.624427	5281.010692	15.967437	-0.053790	3.941770
272.631540	5272.993587	15.972442	-0.053786	3.938904
272.773806	5264.992325	15.977447	-0.053807	3.936044
272.446302	5256.993609	15.982451	-0.053741	3.933175
272.244539	5248.975547	15.987456	-0.053698	3.930299
272.477525	5240.990797	15.992461	-0.053736	3.927441
272.403193	5232.949536	15.997466	-0.053717	3.924554
272.354703	5225.025079	16.002471	-0.053703	3.921708
272.301802	5217.028447	16.007475	-0.053688	3.918834
272.403858	5209.018680	16.012480	-0.053701	3.915956
272.439946	5201.001598	16.017485	-0.053703	3.913072
272.207980	5192.944992	16.022490	-0.053654	3.910167
272.186279	5185.016347	16.027495	-0.053645	3.907309
272.121853	5176.989244	16.032499	-0.053628	3.904413
271.922761	5169.031205	16.037504	-0.053585	3.901537
272.125497	5160.998940	16.042509	-0.053618	3.898640
272.036041	5153.004844	16.047514	-0.053596	3.895749
271.965039	5145.022679	16.052519	-0.053577	3.892861
271.891162	5136.956096	16.057523	-0.053558	3.889940
271.820503	5129.003135	16.062528	-0.053540	3.887057
271.874237	5120.989362	16.067533	-0.053544	3.884153
271.825483	5113.020480	16.072538	-0.053530	3.881261
271.815100	5105.046953	16.077543	-0.053523	3.878366
271.681767	5097.021453	16.082547	-0.053493	3.875448
271.506533	5088.818890	16.087552	-0.053455	3.872462
271.642157	5080.836924	16.092557	-0.053475	3.869560
271.673749	5072.876727	16.097562	-0.053475	3.866662
271.586456	5064.938273	16.102567	-0.053454	3.863767
271.307921	5056.990413	16.107571	-0.053397	3.860863
271.177284	5048.995369	16.112576	-0.053367	3.857942
271.278578	5040.993895	16.117581	-0.053380	3.855022
271.284728	5032.982271	16.122586	-0.053376	3.852093
271.435974	5024.997842	16.127591	-0.053399	3.849176
271.272179	5017.015326	16.132595	-0.053363	3.846250
270.894072	5009.035391	16.137600	-0.053288	3.843319
271.182279	5001.052252	16.142605	-0.053336	3.840397
270.967103	4993.063770	16.147610	-0.053291	3.837462
270.988126	4985.047153	16.152615	-0.053289	3.834518
270.881131	4977.048910	16.157619	-0.053264	3.831577
270.824892	4969.032815	16.162624	-0.053248	3.828627
270.738823	4961.036470	16.167629	-0.053227	3.825682
270.544694	4953.082904	16.172634	-0.053186	3.822749
270.744734	4945.057414	16.177639	-0.053217	3.819794
270.677197	4937.118344	16.182643	-0.053200	3.816864
270.688397	4929.063439	16.187648	-0.053196	3.813890
270.674622	4921.071142	16.192653	-0.053188	3.810937
270.708658	4913.063751	16.197658	-0.053190	3.807977
270.673621	4905.068232	16.202663	-0.053178	3.805017
270.717555	4897.114853	16.207667	-0.053181	3.802072
270.499803	4889.076660	16.212672	-0.053135	3.799088
270.443967	4881.162532	16.217677	-0.053119	3.796151
270.388545	4873.062865	16.222682	-0.053103	3.793143
270.221021	4865.075318	16.227687	-0.053067	3.790172
270.233942	4857.082704	16.232691	-0.053064	3.787201
270.242001	4849.079876	16.237696	-0.053060	3.784223
270.093541	4841.131969	16.242701	-0.053027	3.781260
270.065689	4833.104515	16.247706	-0.053017	3.778267
270.005863	4825.117969	16.252711	-0.053000	3.775287
269.814425	4817.106308	16.257715	-0.052959	3.772292
269.789360	4809.083641	16.262720	-0.052949	3.769294
269.781545	4801.102231	16.267725	-0.052943	3.766310
269.777389	4793.093576	16.272730	-0.052937	3.763313
269.789740	4785.099479	16.277735	-0.052934	3.760320
269.798501	4777.135283	16.282739	-0.052930	3.757335
269.756440	4769.110613	16.287744	-0.052917	3.754324
269.722659	4761.115180	16.292749	-0.052905	3.751322
269.667957	4753.094220	16.297754	-0.052890	3.748308
269.531255	4745.088092	16.302759	-0.052859	3.745294
269.437371	4737.131454	16.307763	-0.052836	3.742298
269.492745	4729.098273	16.312768	-0.052841	3.739274
269.436847	4721.157122	16.317773	-0.052825	3.736280
269.263437	4713.122111	16.322778	-0.052788	3.733245
269.271806	4705.127859	16.327783	-0.052784	3.730227
269.045408	4697.186964	16.332787	-0.052737	3.727222
268.900997	4689.130246	16.337792	-0.052704	3.724172
269.218933	4681.193788	16.342797	-0.052758	3.721176
268.950500	4673.196752	16.347802	-0.052703	3.718141
269.056212	4665.190109	16.352807	-0.052718	3.715108
269.092422	4657.093191	16.357811	-0.052719	3.712037
269.023111	4649.084478	16.362816	-0.052701	3.708995
269.111634	4641.138818	16.367821	-0.052712	3.705978
269.014257	4633.162267	16.372826	-0.052688	3.702942
268.651388	4625.222482	16.377831	-0.052616	3.699911
268.873879	4617.212325	16.382835	-0.052652	3.696865
268.895110	4609.173390	16.387840	-0.052650	3.693801
268.780886	4601.204703	16.392845	-0.052624	3.690758
268.523046	4593.227469	16.397850	-0.052571	3.687705
268.458310	4585.214155	16.402855	-0.052553	3.684641
268.282477	4577.324949	16.407859	-0.052515	3.681619
268.343705	4569.236001	16.412864	-0.052521	3.678524
268.350357	4561.268201	16.417869	-0.052517	3.675471
268.099473	4553.257290	16.422874	-0.052465	3.672393
267.996286	4545.256447	16.427879	-0.052441	3.669319
268.338353	4537.229548	16.432883	-0.052499	3.666245
268.213705	4529.222455	16.437888	-0.052470	3.663163
268.139886	4521.266620	16.442893	-0.052451	3.660100
268.037997	4513.261827	16.447898	-0.052427	3.657015
268.190325	4505.245144	16.452903	-0.052450	3.653930
267.943075	4497.258855	16.457907	-0.052399	3.650842
267.878425	4489.250934	16.462912	-0.052382	3.647749
268.090241	4481.236761	16.467917	-0.052416	3.644658
267.745375	4473.317965	16.472922	-0.052346	3.641587
267.802430	4465.283481	16.477927	-0.052352	3.638478
267.769191	4457.298264	16.482931	-0.052340	3.635384
267.588960	4449.251063	16.487936	-0.052301	3.632259
267.714435	4441.271890	16.492941	-0.052319	3.629166
267.541736	4433.280649	16.497946	-0.052282	3.626058
267.861643	4425.275139	16.502951	-0.052336	3.622955
267.654957	4417.293602	16.507955	-0.052292	3.619844
267.387642	4409.351289	16.512960	-0.052237	3.616744
267.686684	4401.311572	16.517965	-0.052288	3.613619
267.492508	4393.273957	16.522970	-0.052246	3.610479
267.588912	4385.306991	16.527975	-0.052259	3.607371
267.549193	4377.331663	16.532979	-0.052246	3.604254
267.264514	4369.365364	16.537984	-0.052188	3.601131
267.323306	4361.396184	16.542989	-0.052193	3.598013
267.279647	4353.363884	16.547994	-0.052180	3.594865
267.119030	4345.378793	16.552999	-0.052145	3.591730
267.130644	4337.378141	16.558003	-0.052142	3.588590
267.033577	4329.402587	16.563008	-0.052118	3.585455
267.224341	4321.392795	16.568013	-0.052148	3.582311
266.969189	4313.388684	16.573018	-0.052096	3.579154
267.001278	4305.428906	16.578023	-0.052096	3.576021
267.065431	4297.439737	16.583027	-0.052103	3.572873
266.823165	4289.361924	16.588032	-0.052053	3.569679
266.899283	4281.442192	16.593037	-0.052061	3.566554
266.746627	4273.443389	16.598042	-0.052028	3.563389
266.647400	4265.426567	16.603047	-0.052004	3.560214
266.514461	4257.490350	16.608051	-0.051974	3.557068
266.659701	4249.388029	16.613056	-0.051996	3.553862
266.784936	4241.335344	16.618061	-0.052014	3.550671
266.443690	4233.377726	16.623066	-0.051945	3.547502
266.397255	4225.397710	16.628071	-0.051931	3.544330
266.658209	4217.438938	16.633075	-0.051974	3.541172
266.412691	4209.444081	16.638080	-0.051923	3.537983
266.301734	4201.455131	16.643085	-0.051897	3.534796
266.142494	4193.466097	16.648090	-0.051862	3.531606
266.225465	4185.459947	16.653095	-0.051872	3.528413
265.938699	4177.491148	16.658099	-0.051814	3.525220
265.932328	4169.486722	16.663104	-0.051807	3.522019
266.114369	4161.483923	16.668109	-0.051836	3.518822
266.063668	4153.472454	16.673114	-0.051821	3.515611
265.989319	4145.481026	16.678119	-0.051802	3.512404
265.717657	4137.493299	16.683123	-0.051746	3.509190
265.780845	4129.465707	16.688128	-0.051752	3.505967
265.837843	4121.507260	16.693133	-0.051758	3.502769
265.834823	4113.503286	16.698138	-0.051752	3.499548
265.755638	4105.538887	16.703143	-0.051732	3.496337
265.725166	4097.556418	16.708147	-0.051721	3.493118
265.611442	4089.534410	16.713152	-0.051694	3.489877
265.661365	4081.576755	16.718157	-0.051698	3.486664
265.616722	4073.585913	16.723162	-0.051685	3.483432
265.450870	4065.607330	16.728167	-0.051649	3.480198
265.436429	4057.632895	16.733171	-0.051641	3.476967
265.179403	4049.610218	16.738176	-0.051588	3.473706
265.146070	4041.606863	16.743181	-0.051576	3.470457
265.028211	4033.583873	16.748186	-0.051549	3.467194
265.138921	4025.586539	16.753191	-0.051564	3.463946
265.176244	4017.613197	16.758195	-0.051566	3.460702
265.037447	4009.644426	16.763200	-0.051535	3.457452
264.954854	4001.642784	16.768205	-0.051514	3.454186
264.956005	3993.600028	16.773210	-0.051509	3.450904
264.955289	3985.641465	16.778215	-0.051503	3.447653
264.830203	3977.632451	16.783219	-0.051475	3.444373
264.905895	3969.662286	16.788224	-0.051484	3.441114
264.979103	3961.660998	16.793229	-0.051492	3.437838
264.659012	3953.677710	16.798234	-0.051427	3.434554
264.611593	3945.656608	16.803239	-0.051413	3.431260
264.745506	3937.661963	16.808243	-0.051433	3.427980
264.525390	3929.662691	16.813248	-0.051386	3.424682
264.581568	3921.736671	16.818253	-0.051391	3.421421
264.514661	3913.722206	16.823258	-0.051374	3.418117
264.504664	3905.713143	16.828263	-0.051367	3.414813
264.401201	3897.701365	16.833267	-0.051342	3.411502
264.474034	3889.695010	16.838272	-0.051350	3.408196
264.484196	3881.734752	16.843277	-0.051347	3.404903
264.413872	3873.760954	16.848282	-0.051328	3.401599
264.243433	3865.805487	16.853287	-0.051291	3.398296
264.389628	3857.804492	16.858291	-0.051313	3.394982
264.149271	3849.705130	16.863296	-0.051263	3.391610
264.185444	3841.731268	16.868301	-0.051265	3.388297
264.269496	3833.730445	16.873306	-0.051275	3.384971
264.002222	3825.814073	16.878311	-0.051220	3.381664
264.020578	3817.825464	16.883315	-0.051218	3.378334
264.064610	3809.799199	16.888320	-0.051221	3.374986
264.101518	3801.809869	16.893325	-0.051223	3.371650
263.825023	3793.825820	16.898330	-0.051166	3.368302
263.621410	3785.842181	16.903335	-0.051123	3.364953
263.733863	3777.878480	16.908339	-0.051138	3.361620
263.482880	3769.873207	16.913344	-0.051086	3.358253
263.693422	3761.908811	16.918349	-0.051120	3.354917
263.640726	3753.861143	16.923354	-0.051105	3.351533
263.690351	3745.868497	16.928359	-0.051109	3.348173
263.764965	3737.869854	16.933363	-0.051118	3.344807
263.758673	3729.887676	16.938368	-0.051111	3.341442
263.670937	3721.918354	16.943373	-0.051089	3.338076
263.482113	3713.931135	16.948378	-0.051049	3.334696
263.251381	3705.940983	16.953383	-0.051001	3.331309
263.264624	3697.968843	16.958387	-0.050998	3.327936
263.136479	3689.927976	16.963392	-0.050969	3.324524
263.024034	3682.019874	16.968397	-0.050943	3.321166
262.932570	3674.023176	16.973402	-0.050920	3.317768
262.851125	3666.015485	16.978407	-0.050900	3.314362
263.003893	3657.940484	16.983411	-0.050923	3.310932
262.962279	3649.937788	16.988416	-0.050910	3.307523
262.919636	3641.996895	16.993421	-0.050897	3.304136
262.800907	3634.013128	16.998426	-0.050869	3.300725
262.776331	3626.060013	17.003431	-0.050859	3.297326
262.927570	3618.047689	17.008435	-0.050882	3.293906
262.599116	3610.043306	17.013440	-0.050816	3.290467
262.507461	3602.086043	17.018445	-0.050793	3.287054
262.752309	3594.065548	17.023450	-0.050834	3.283623
262.449966	3586.093626	17.028455	-0.050772	3.280188
262.501931	3578.151383	17.033459	-0.050776	3.276776
262.504594	3570.095653	17.038464	-0.050772	3.273309
262.490526	3562.081840	17.043469	-0.050764	3.269857
262.455986	3554.123940	17.048474	-0.050752	3.266424
262.296727	3546.140183	17.053479	-0.050717	3.262971
262.203232	3538.169819	17.058483	-0.050694	3.259523
262.080185	3530.191873	17.063488	-0.050666	3.256067
262.058756	3522.170686	17.068493	-0.050657	3.252593
262.030318	3514.160885	17.073498	-0.050646	3.249119
261.987970	3506.173163	17.078503	-0.050633	3.245651
261.917002	3498.203812	17.083507	-0.050615	3.242186
261.838511	3490.227926	17.088512	-0.050595	3.238714
262.113561	3482.253867	17.093517	-0.050641	3.235253
262.132583	3474.165083	17.098522	-0.050639	3.231728
262.030960	3466.166362	17.103527	-0.050615	3.228234
262.082104	3458.196482	17.108531	-0.050619	3.224755
261.887343	3450.258742	17.113536	-0.050577	3.221276
261.876384	3442.262666	17.118541	-0.050570	3.217775
261.615099	3434.311471	17.123546	-0.050516	3.214280
261.676921	3426.254922	17.128551	-0.050522	3.210748
261.634438	3418.320712	17.133555	-0.050509	3.207262
261.633967	3410.299659	17.138560	-0.050504	3.203735
261.607041	3402.359404	17.143565	-0.050493	3.200239
261.486482	3394.389224	17.148570	-0.050466	3.196722
261.308761	3386.366079	17.153575	-0.050427	3.193176
261.259972	3378.362345	17.158579	-0.050413	3.189639
261.209427	3370.366270	17.163584	-0.050398	3.186102
261.087686	3362.411956	17.168589	-0.050370	3.182576
261.085994	3354.417764	17.173594	-0.050364	3.179034
261.110618	3346.420126	17.178599	-0.050364	3.175488
261.004789	3338.425622	17.183603	-0.050339	3.171933
260.887950	3330.418029	17.188608	-0.050312	3.168368
261.160447	3322.417179	17.193613	-0.050357	3.164818
260.918220	3314.470496	17.198618	-0.050307	3.161267
260.934054	3306.498894	17.203623	-0.050304	3.157712
260.916221	3298.498295	17.208627	-0.050296	3.154138
260.810821	3290.485940	17.213632	-0.050271	3.150551
260.811985	3282.491949	17.218637	-0.050266	3.146973
260.668260	3274.508601	17.223642	-0.050234	3.143389
260.695734	3266.497591	17.228647	-0.050234	3.139797
260.628441	3258.570984	17.233651	-0.050216	3.136233
260.581408	3250.544579	17.238656	-0.050202	3.132622
260.588671	3242.574120	17.243661	-0.050198	3.129034
260.474492	3234.577645	17.248666	-0.050171	3.125425
260.240088	3226.648625	17.253671	-0.050122	3.121837
260.209715	3218.667981	17.258675	-0.050111	3.118231
260.227947	3210.640045	17.263680	-0.050109	3.114601
260.189202	3202.640882	17.268685	-0.050097	3.110977
260.184818	3194.660045	17.273690	-0.050091	3.107359
260.171647	3186.644694	17.278695	-0.050083	3.103721
260.212858	3178.668360	17.283699	-0.050085	3.100098
259.873667	3170.767386	17.288704	-0.050017	3.096488
260.067500	3162.734168	17.293709	-0.050048	3.092838
260.005829	3154.705807	17.298714	-0.050031	3.089175
259.849319	3146.752561	17.303719	-0.049997	3.085537
259.885520	3138.792823	17.308723	-0.049998	3.081900
259.652664	3130.803418	17.313728	-0.049949	3.078233
259.481717	3122.835797	17.318733	-0.049912	3.074575
259.519022	3114.725419	17.323738	-0.049914	3.070856
259.592427	3106.742800	17.328743	-0.049922	3.067194
259.475343	3098.797833	17.333747	-0.049895	3.063535
259.277386	3090.829976	17.338752	-0.049853	3.059858
259.422521	3082.870023	17.343757	-0.049875	3.056196
259.365752	3074.855630	17.348762	-0.049859	3.052494
259.274451	3066.857221	17.353767	-0.049837	3.048795
259.285296	3058.889132	17.358771	-0.049833	3.045109
259.334022	3050.928820	17.363776	-0.049837	3.041424
259.299351	3042.955756	17.368781	-0.049825	3.037725
259.041788	3034.981788	17.373786	-0.049772	3.034011
258.890044	3026.961828	17.378791	-0.049738	3.030275
259.044538	3018.977818	17.383795	-0.049762	3.026567
258.864133	3011.010096	17.388800	-0.049723	3.022845
258.799573	3003.036244	17.393805	-0.049706	3.019121
258.781642	2995.063408	17.398810	-0.049697	3.015396
258.722708	2987.023996	17.403815	-0.049681	3.011633
258.731542	2979.061540	17.408819	-0.049677	3.007904
258.587776	2971.067693	17.413824	-0.049645	3.004149
258.516989	2963.121460	17.418829	-0.049627	3.000414
258.444074	2955.154187	17.423834	-0.049608	2.996665
258.512764	2947.126349	17.428839	-0.049615	2.992890
258.566862	2939.113453	17.433843	-0.049620	2.989117
258.153412	2931.163973	17.438848	-0.049538	2.985345
258.234774	2923.190917	17.443853	-0.049548	2.981582
258.226029	2915.205775	17.448858	-0.049541	2.977804
258.151126	2907.215399	17.453863	-0.049522	2.974016
258.281265	2899.213442	17.458867	-0.049540	2.970227
258.116546	2891.240558	17.463872	-0.049504	2.966433
258.167990	2883.274577	17.468877	-0.049509	2.962648
257.883631	2875.321890	17.473882	-0.049451	2.958847
257.901696	2867.334087	17.478887	-0.049449	2.955040
257.958691	2859.324286	17.483891	-0.049454	2.951219
257.684530	2851.324527	17.488896	-0.049398	2.947382
257.747906	2843.332880	17.493901	-0.049404	2.943561
257.730669	2835.364183	17.498906	-0.049396	2.939741
257.670363	2827.409858	17.503911	-0.049379	2.935921
257.573859	2819.408146	17.508915	-0.049356	2.932072
257.627716	2811.396792	17.513920	-0.049361	2.928221
257.911873	2803.410431	17.518925	-0.049408	2.924388
257.643475	2795.508130	17.523930	-0.049353	2.920563
257.434846	2787.535519	17.528935	-0.049309	2.916701
257.635280	2779.465019	17.533939	-0.049341	2.912808
257.491046	2771.447436	17.538944	-0.049309	2.908918
257.177683	2763.495232	17.543949	-0.049245	2.905045
257.373022	2755.525551	17.548954	-0.049276	2.901186
257.280879	2747.550523	17.553959	-0.049254	2.897303
257.151526	2739.592899	17.558963	-0.049224	2.893422
257.025381	2731.572076	17.563968	-0.049195	2.889505
257.039516	2723.614421	17.568973	-0.049193	2.885621
257.090662	2715.666563	17.573978	-0.049197	2.881738
256.684741	2707.729141	17.578983	-0.049116	2.877831
256.792917	2699.729637	17.583987	-0.049131	2.873916
256.711538	2691.680734	17.588992	-0.049111	2.869960
256.521267	2683.732562	17.593997	-0.049070	2.866043
256.738513	2675.739026	17.599002	-0.049105	2.862121
256.576414	2667.765897	17.604007	-0.049070	2.858182
256.590147	2659.818257	17.609011	-0.049067	2.854260
256.488157	2651.804900	17.614016	-0.049043	2.850294
256.509713	2643.830450	17.619021	-0.049041	2.846348
256.454792	2635.864338	17.624026	-0.049026	2.842397
256.316014	2627.897433	17.629031	-0.048995	2.838435
256.587273	2619.913535	17.634035	-0.049040	2.834482
256.346368	2611.903396	17.639040	-0.048990	2.830482
256.348878	2603.914007	17.644045	-0.048985	2.826500
256.188425	2595.964410	17.649050	-0.048950	2.822524
256.132738	2587.985457	17.654055	-0.048934	2.818532
256.076094	2580.025425	17.659059	-0.048918	2.814545
255.977916	2572.022945	17.664064	-0.048895	2.810528
256.065806	2564.033648	17.669069	-0.048906	2.806523
256.045566	2556.047009	17.674074	-0.048897	2.802507
255.980770	2548.088104	17.679079	-0.048879	2.798497
255.900270	2540.147400	17.684083	-0.048859	2.794489
255.930265	2532.126911	17.689088	-0.048859	2.790442
255.787202	2524.149135	17.694093	-0.048827	2.786400
255.844406	2516.184492	17.699098	-0.048833	2.782371
255.635105	2508.224089	17.704103	-0.048789	2.778322
255.662050	2500.267029	17.709107	-0.048788	2.774283
255.582780	2492.251685	17.714112	-0.048768	2.770203
255.456566	2484.295316	17.719117	-0.048739	2.766143
255.476678	2476.329346	17.724122	-0.048738	2.762081
255.163166	2468.389634	17.729127	-0.048674	2.758007
255.359969	2460.375877	17.734131	-0.048706	2.753919
255.226676	2452.316391	17.739136	-0.048675	2.749782
255.178336	2444.349122	17.744141	-0.048661	2.745692
255.267005	2436.391599	17.749146	-0.048672	2.741608
255.146353	2428.425684	17.754151	-0.048645	2.737501
255.097785	2420.478415	17.759155	-0.048630	2.733403
254.892220	2412.483684	17.764160	-0.048587	2.729263
254.878661	2404.504412	17.769165	-0.048579	2.725138
255.004769	2396.553806	17.774170	-0.048597	2.721029
254.917553	2388.578507	17.779175	-0.048576	2.716888
254.892163	2380.611062	17.784179	-0.048566	2.712749
254.754373	2372.608605	17.789184	-0.048535	2.708579
254.486076	2364.655091	17.794189	-0.048479	2.704419
254.683342	2356.673846	17.799194	-0.048511	2.700267
254.769122	2348.673335	17.804199	-0.048521	2.696092
254.559335	2340.739696	17.809203	-0.048477	2.691927
254.297001	2332.774178	17.814208	-0.048423	2.687735
254.517269	2324.770286	17.819213	-0.048459	2.683548
254.456974	2316.828005	17.824218	-0.048442	2.679368
254.282340	2308.865748	17.829223	-0.048404	2.675164
254.449161	2300.847608	17.834227	-0.048430	2.670945
254.424124	2292.854054	17.839232	-0.048420	2.666721
253.986087	2284.945687	17.844237	-0.048333	2.662508
254.093975	2276.961382	17.849242	-0.048348	2.658284
254.077755	2268.978950	17.854247	-0.048340	2.654046
254.135216	2260.970661	17.859251	-0.048345	2.649792
253.924181	2253.034047	17.864256	-0.048301	2.645552
253.910793	2245.073239	17.869261	-0.048293	2.641305
253.959624	2237.112948	17.874266	-0.048297	2.637056
253.765788	2229.127890	17.879271	-0.048255	2.632770
253.676562	2221.150367	17.884275	-0.048234	2.628489
253.564168	2213.182931	17.889280	-0.048207	2.624204
253.709071	2205.206718	17.894285	-0.048229	2.619925
253.519856	2197.278616	17.899290	-0.048189	2.615642
253.409215	2189.266867	17.904295	-0.048163	2.611313
253.589275	2181.276338	17.909299	-0.048191	2.607007
253.392321	2173.328663	17.914304	-0.048149	2.602692
253.351289	2165.376638	17.919309	-0.048136	2.598378
253.327333	2157.381434	17.924314	-0.048126	2.594034
253.148875	2149.239120	17.929319	-0.048088	2.589593
253.035611	2141.317978	17.934323	-0.048061	2.585268
253.049047	2133.388026	17.939328	-0.048058	2.580941
253.289120	2125.407043	17.944333	-0.048098	2.576594
253.027488	2117.495176	17.949338	-0.048044	2.572242
253.105527	2109.498466	17.954343	-0.048053	2.567861
253.068922	2101.554183	17.959347	-0.048041	2.563492
253.034745	2093.604736	17.964352	-0.048029	2.559114
252.960821	2085.656389	17.969357	-0.048010	2.554726
252.973829	2077.668965	17.974362	-0.048008	2.550315
252.998291	2069.665149	17.979367	-0.048007	2.545887
252.882141	2061.760307	17.984371	-0.047980	2.541498
252.674322	2053.803301	17.989376	-0.047936	2.537065
252.598392	2045.844116	17.994381	-0.047917	2.532632
252.457375	2037.880604	17.999386	-0.047885	2.528185
252.350456	2029.905603	18.004391	-0.047860	2.523725
252.375504	2021.966391	18.009395	-0.047859	2.519288
252.144799	2013.998693	18.014400	-0.047811	2.514808
252.198868	2005.964100	18.019405	-0.047816	2.510303
252.284436	1998.001713	18.024410	-0.047826	2.505832
252.004664	1990.055841	18.029415	-0.047769	2.501337
251.990949	1982.128324	18.034419	-0.047761	2.496863
251.777433	1974.152201	18.039424	-0.047716	2.492339
251.902901	1966.160147	18.044429	-0.047734	2.487823
251.840810	1958.199347	18.049434	-0.047717	2.483302
251.780305	1950.249578	18.054439	-0.047701	2.478780
251.794598	1942.291775	18.059443	-0.047698	2.474250
251.531143	1934.332106	18.064448	-0.047644	2.469690
251.479154	1926.359246	18.069453	-0.047629	2.465130
251.565712	1918.413628	18.074458	-0.047640	2.460587
251.422321	1910.447364	18.079463	-0.047608	2.456007
251.393309	1902.489242	18.084467	-0.047597	2.451431
251.548066	1894.482398	18.089472	-0.047621	2.446833
251.373165	1886.551539	18.094477	-0.047583	2.442245
251.428343	1878.611701	18.099482	-0.047588	2.437661
251.219977	1870.616346	18.104487	-0.047544	2.433016
251.214118	1862.607583	18.109491	-0.047537	2.428369
251.137040	1854.647412	18.114496	-0.047518	2.423737
251.135249	1846.696581	18.119501	-0.047512	2.419106
251.124625	1838.761865	18.124506	-0.047505	2.414476
251.158675	1830.765760	18.129511	-0.047506	2.409804
250.925423	1822.851989	18.134515	-0.047457	2.405151
250.701131	1814.922989	18.139520	-0.047410	2.400480
250.756920	1806.973375	18.144525	-0.047415	2.395810
250.716012	1798.985919	18.149530	-0.047402	2.391101
250.458006	1791.026261	18.154535	-0.047349	2.386382
250.748344	1783.055414	18.159539	-0.047398	2.381690
250.486549	1775.123136	18.164544	-0.047344	2.376968
250.485294	1767.146412	18.169549	-0.047338	2.372231
250.419130	1759.196416	18.174554	-0.047321	2.367496
250.452964	1751.224605	18.179559	-0.047322	2.362745
250.507883	1743.291537	18.184563	-0.047327	2.358010
250.411013	1735.327076	18.189568	-0.047303	2.353235
250.315100	1727.343872	18.194573	-0.047280	2.348438
250.369546	1719.388628	18.199578	-0.047285	2.343661
250.018861	1711.478480	18.204583	-0.047215	2.338868
250.238994	1703.513114	18.209587	-0.047250	2.334079
249.906664	1695.560774	18.214592	-0.047183	2.329242
249.894764	1687.601437	18.219597	-0.047176	2.324417
249.844458	1679.671808	18.224602	-0.047161	2.319597
249.827289	1671.705997	18.229607	-0.047152	2.314748
249.787493	1663.730306	18.234611	-0.047140	2.309881
249.599172	1655.793779	18.239616	-0.047099	2.305014
249.559968	1647.850921	18.244621	-0.047087	2.300147
249.520984	1639.920034	18.249626	-0.047074	2.295276
249.372455	1631.939647	18.254631	-0.047041	2.290355
249.484997	1623.972750	18.259635	-0.047057	2.285454
249.469755	1616.025294	18.264640	-0.047049	2.280543
249.318914	1608.113893	18.269645	-0.047016	2.275633
249.180164	1600.101615	18.274650	-0.046985	2.270651
249.010661	1592.133076	18.279655	-0.046948	2.265682
249.034654	1584.195883	18.284659	-0.046947	2.260738
249.169937	1576.228886	18.289664	-0.046967	2.255774
248.923336	1568.304164	18.294669	-0.046916	2.250793
248.844179	1560.361442	18.299674	-0.046896	2.245804
248.648689	1552.437224	18.304679	-0.046854	2.240806
248.908488	1544.471564	18.309683	-0.046897	2.235810
248.966827	1536.489404	18.314688	-0.046903	2.230774
248.856465	1528.532528	18.319693	-0.046877	2.225729
248.934120	1520.608004	18.324698	-0.046886	2.220709
248.616244	1512.702804	18.329703	-0.046822	2.215655
248.504570	1504.761467	18.334707	-0.046796	2.210584
248.467698	1496.796166	18.339712	-0.046783	2.205493
248.462924	1488.859120	18.344717	-0.046777	2.200412
248.481398	1480.941981	18.349722	-0.046775	2.195334
248.357838	1472.945839	18.354727	-0.046747	2.190180
248.406858	1464.998864	18.359731	-0.046751	2.185061
248.378085	1457.054926	18.364736	-0.046740	2.179925
248.184932	1449.144339	18.369741	-0.046699	2.174784
248.146791	1441.189522	18.374746	-0.046687	2.169615
248.066919	1433.249297	18.379751	-0.046667	2.164441
247.938445	1425.347206	18.384755	-0.046637	2.159274
247.813309	1417.404978	18.389760	-0.046609	2.154068
247.733906	1409.427690	18.394765	-0.046589	2.148832
247.707828	1401.499759	18.399770	-0.046579	2.143620
247.448566	1393.592040	18.404775	-0.046525	2.138386
247.502898	1385.639337	18.409779	-0.046530	2.133140
247.466202	1377.676096	18.414784	-0.046518	2.127865
247.409953	1369.752804	18.419789	-0.046502	2.122601
247.514145	1361.828925	18.424794	-0.046516	2.117340
247.411776	1353.841483	18.429799	-0.046492	2.112003
247.371622	1345.877907	18.434803	-0.046479	2.106675
247.328651	1337.948619	18.439808	-0.046466	2.101355
247.161729	1330.050847	18.444813	-0.046430	2.096032
247.014138	1322.124398	18.449818	-0.046397	2.090677
246.961215	1314.171386	18.454823	-0.046382	2.085300
247.068932	1306.251038	18.459827	-0.046397	2.079947
246.767413	1298.365463	18.464832	-0.046335	2.074563
246.750772	1290.390852	18.469837	-0.046327	2.069133
246.843874	1282.446754	18.474842	-0.046339	2.063720
246.538036	1274.552695	18.479847	-0.046277	2.058287
246.630951	1266.602105	18.484851	-0.046289	2.052841
246.407832	1258.690213	18.489856	-0.046242	2.047376
246.480041	1250.742312	18.494861	-0.046250	2.041901
246.511974	1242.834405	18.499866	-0.046251	2.036434
246.411099	1234.876608	18.504871	-0.046227	2.030905
246.440415	1226.945371	18.509875	-0.046227	2.025393
246.464161	1219.011461	18.514880	-0.046226	2.019863
246.210940	1211.129385	18.519885	-0.046174	2.014325
246.058745	1203.208218	18.524890	-0.046140	2.008755
245.983891	1195.263757	18.529895	-0.046121	2.003162
246.103721	1187.340330	18.534899	-0.046138	1.997587
246.015204	1179.414891	18.539904	-0.046116	1.991974
245.899513	1171.483553	18.544909	-0.046089	1.986338
245.963141	1163.562166	18.549914	-0.046096	1.980712
245.765221	1155.666068	18.554919	-0.046054	1.975061
245.707376	1147.742186	18.559923	-0.046038	1.969388
245.786549	1139.803103	18.564928	-0.046047	1.963702
245.613227	1131.922698	18.569933	-0.046010	1.958015
245.647062	1123.965381	18.574938	-0.046011	1.952278
245.243849	1116.062617	18.579943	-0.045931	1.946516
245.353854	1108.124614	18.584947	-0.045946	1.940768
245.254895	1100.218265	18.589952	-0.045922	1.935002
245.236180	1092.289943	18.594957	-0.045913	1.929213
245.230788	1084.379781	18.599962	-0.045907	1.923420
244.926620	1076.510242	18.604967	-0.045845	1.917607
245.022770	1068.570927	18.609971	-0.045858	1.911769
244.999755	1060.636006	18.614976	-0.045848	1.905903
244.804603	1052.742721	18.619981	-0.045807	1.900030
244.717625	1044.863658	18.624986	-0.045785	1.894162
244.830909	1036.902179	18.629991	-0.045801	1.888237
244.651790	1029.038730	18.634995	-0.045763	1.882334
244.636520	1021.129043	18.640000	-0.045755	1.876395
244.586138	1013.198591	18.645005	-0.045740	1.870419
244.587429	1005.280456	18.650010	-0.045735	1.864438
244.312316	997.410359	18.655015	-0.045679	1.858443
244.228897	989.510312	18.660019	-0.045658	1.852427
244.377036	981.560260	18.665024	-0.045680	1.846381
244.442109	973.652885	18.670029	-0.045687	1.840338
244.373940	965.781888	18.675034	-0.045669	1.834287
244.183194	957.879645	18.680039	-0.045628	1.828178
244.024317	949.996223	18.685043	-0.045593	1.822066
244.043343	942.100894	18.690048	-0.045592	1.815946
243.777220	934.214819	18.695053	-0.045537	1.809778
243.935427	926.307463	18.700058	-0.045561	1.803623
243.754272	918.434628	18.705063	-0.045522	1.797433
243.732184	910.504346	18.710067	-0.045513	1.791196
243.612068	902.594733	18.715072	-0.045485	1.784942
243.555297	894.715675	18.720077	-0.045469	1.778698
243.612121	886.814474	18.725082	-0.045475	1.772427
243.434484	878.924450	18.730087	-0.045437	1.766115
243.362281	871.068336	18.735091	-0.045418	1.759820
243.458177	863.171831	18.740096	-0.045430	1.753491
243.312284	855.276491	18.745101	-0.045398	1.747110
243.413961	847.390064	18.750106	-0.045412	1.740744
243.206638	839.538105	18.755111	-0.045368	1.734343
242.957603	831.680326	18.760115	-0.045316	1.727908
243.048691	823.779961	18.765120	-0.045328	1.721458
242.912358	815.922974	18.770125	-0.045298	1.714990
242.652106	808.066045	18.775130	-0.045244	1.708481
242.519218	800.175313	18.780135	-0.045214	1.701936
242.616552	792.286959	18.785139	-0.045227	1.695398
242.409705	784.426450	18.790144	-0.045183	1.688818
242.190174	776.582164	18.795149	-0.045137	1.682224
242.309441	768.692367	18.800154	-0.045154	1.675610
242.237725	760.801934	18.805159	-0.045135	1.668945
242.250441	752.935342	18.810163	-0.045132	1.662284
242.256718	745.067337	18.815168	-0.045128	1.655594
242.090489	737.211242	18.820173	-0.045092	1.648864
241.964007	729.376276	18.825178	-0.045064	1.642130
241.784410	721.537287	18.830183	-0.045025	1.635357
241.817608	713.597272	18.835187	-0.045026	1.628498
241.688309	705.759102	18.840192	-0.044997	1.621676
241.508746	697.925216	18.845197	-0.044958	1.614822
241.589705	690.052197	18.850202	-0.044968	1.607941
241.470450	682.203556	18.855207	-0.044940	1.601023
241.346335	674.388614	18.860211	-0.044912	1.594105
241.421409	666.497836	18.865216	-0.044921	1.587117
241.524280	658.629310	18.870221	-0.044935	1.580122
241.449010	650.818749	18.875226	-0.044916	1.573123
241.235257	642.985064	18.880231	-0.044871	1.566051
241.363857	635.146112	18.885235	-0.044889	1.558992
241.119512	627.340246	18.890240	-0.044839	1.551877
240.887593	619.509905	18.895245	-0.044790	1.544708
241.036291	611.654564	18.900250	-0.044813	1.537539
240.735644	603.849264	18.905255	-0.044752	1.530316
240.707863	596.018537	18.910259	-0.044741	1.523076
240.774167	588.186035	18.915264	-0.044748	1.515813
240.524455	580.371765	18.920269	-0.044697	1.508485
240.580464	572.538842	18.925274	-0.044702	1.501150
240.410207	564.748088	18.930279	-0.044665	1.493784
240.427592	556.909940	18.935283	-0.044663	1.486366
240.389706	549.121975	18.940288	-0.044651	1.478950
240.060064	541.314823	18.945293	-0.044584	1.471432
240.062547	533.482708	18.950298	-0.044580	1.463903
239.945242	525.683210	18.955303	-0.044553	1.456349
239.853757	517.879581	18.960307	-0.044530	1.448755
239.616128	510.108397	18.965312	-0.044481	1.441129
239.757410	502.283903	18.970317	-0.044502	1.433472
239.855045	494.459381	18.975322	-0.044515	1.425766
239.751590	486.692243	18.980327	-0.044491	1.418042
239.749523	478.902457	18.985331	-0.044485	1.410271
239.679207	471.128619	18.990336	-0.044467	1.402460
239.439344	463.389579	18.995341	-0.044417	1.394613
239.290488	455.607228	19.000346	-0.044384	1.386693
239.105429	447.846743	19.005351	-0.044345	1.378743
239.109326	440.059824	19.010355	-0.044340	1.370752
239.128137	432.285684	19.015360	-0.044338	1.362731
238.935827	424.545730	19.020365	-0.044298	1.354660
239.009824	416.760658	19.025370	-0.044306	1.346541
238.869626	409.027201	19.030375	-0.044275	1.338389
238.811486	401.277517	19.035379	-0.044259	1.330184
238.994421	393.505819	19.040384	-0.044288	1.321948
238.469005	385.809301	19.045389	-0.044185	1.313613
238.402790	377.971451	19.050394	-0.044167	1.305156
238.289907	370.255875	19.055399	-0.044141	1.296768
238.119793	362.551595	19.060403	-0.044104	1.288327
238.018675	354.842943	19.065408	-0.044081	1.279838
237.977145	347.123043	19.070413	-0.044068	1.271291
237.990716	339.408973	19.075418	-0.044065	1.262703
237.843328	331.716233	19.080423	-0.044033	1.254050
237.762299	324.008985	19.085427	-0.044012	1.245333
237.929034	316.307325	19.090432	-0.044038	1.236609
237.633605	308.635534	19.095437	-0.043978	1.227767
237.567607	300.960387	19.100442	-0.043961	1.218902
237.522690	293.272334	19.105447	-0.043947	1.209961
237.378584	285.615181	19.110451	-0.043915	1.200970
237.049202	278.010530	19.115456	-0.043849	1.191936
236.784184	270.370312	19.120461	-0.043795	1.182803
236.492814	262.758819	19.125466	-0.043735	1.173628
236.093251	255.145647	19.130471	-0.043656	1.164357
235.796364	247.538369	19.135475	-0.043596	1.155039
235.539673	239.884273	19.140480	-0.043543	1.145596
235.030918	232.315238	19.145485	-0.043443	1.136127
234.755478	224.707047	19.150490	-0.043387	1.126579
234.569493	217.106200	19.155495	-0.043347	1.116978
234.101368	209.549440	19.160499	-0.043255	1.107288
233.753657	201.983378	19.165504	-0.043185	1.097527
233.292420	194.434505	19.170509	-0.043094	1.087675
232.921988	186.900546	19.175514	-0.043020	1.077772
232.574161	179.333745	19.180519	-0.042950	1.067740
232.271363	171.791198	19.185523	-0.042889	1.057655
231.843215	164.276141	19.190528	-0.042804	1.047480
231.295709	156.794187	19.195533	-0.042697	1.037222
230.902951	149.295029	19.200538	-0.042619	1.026875
230.507386	141.804749	19.205543	-0.042541	1.016434
230.115789	134.325757	19.210547	-0.042463	1.005901
229.676523	126.876961	19.215552	-0.042376	0.995288
229.278500	119.381505	19.220557	-0.042297	0.984503
228.949301	111.938046	19.225562	-0.042231	0.973691
228.308633	104.542279	19.230567	-0.042106	0.962748
227.970523	97.126174	19.235571	-0.042039	0.951727
227.602274	89.724129	19.240576	-0.041965	0.940590
227.240052	82.333041	19.245581	-0.041893	0.929337
226.682610	75.010477	19.250586	-0.041784	0.917999
226.163689	67.666264	19.255591	-0.041683	0.906496
225.754036	60.566853	19.260595	-0.041602	0.895260