Tue Mar 23 10:39:42 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.747023	-0.182216	0.000000	-0.000030	0.720567

0.670444	-0.182766	0.005005	-0.000016	0.720539
0.688322	-0.182061	0.010010	-0.000019	0.720546
0.429167	-0.138769	0.015014	0.000029	0.720540
0.766730	-0.197242	0.020019	-0.000034	0.720544
0.891354	-0.220220	0.025024	-0.000057	0.720542
0.580334	-0.167772	0.030029	0.000001	0.720536
0.726606	-0.186797	0.035034	-0.000026	0.720550
0.784557	-0.202738	0.040038	-0.000037	0.720539
0.675467	-0.181290	0.045043	-0.000016	0.720543
0.726469	-0.191873	0.050048	-0.000026	0.720540
0.868877	-0.219958	0.055053	-0.000052	0.720534
0.832806	-0.210203	0.060058	-0.000045	0.720541
0.646367	-0.180571	0.065062	-0.000011	0.720533
0.869816	-0.264816	0.070067	-0.000052	0.720446
0.764762	-0.358117	0.075072	-0.000033	0.720225
0.414221	-0.297917	0.080077	0.000033	0.720221
0.455985	-0.299129	0.085082	0.000025	0.720233
0.603501	-0.331848	0.090086	-0.000002	0.720220
0.385789	-0.289594	0.095091	0.000038	0.720227
0.605650	-0.330321	0.100096	-0.000003	0.720224
0.866051	-0.451863	0.105101	-0.000051	0.720075
0.937733	-0.547510	0.110106	-0.000064	0.719912
0.728541	-0.517980	0.115110	-0.000025	0.719897
0.817734	-0.528710	0.120115	-0.000042	0.719907
0.805308	-0.526493	0.125120	-0.000040	0.719907
0.684070	-0.615877	0.130125	-0.000017	0.719688
0.831784	-0.682629	0.135130	-0.000044	0.719608
0.691931	-0.661365	0.140134	-0.000018	0.719601
0.693703	-0.661399	0.145139	-0.000018	0.719601
0.238596	-0.655159	0.150144	0.000066	0.719454
0.474313	-0.791019	0.155149	0.000023	0.719268
0.444522	-0.783614	0.160154	0.000028	0.719272
0.353604	-0.771535	0.165158	0.000045	0.719264
0.401175	-0.858009	0.170163	0.000036	0.719110
0.659995	-0.978129	0.175168	-0.000012	0.718964
0.521250	-0.955040	0.180173	0.000014	0.718961
0.443192	-0.943826	0.185178	0.000029	0.718955
0.545414	-1.118905	0.190182	0.000010	0.718646
0.708236	-1.146867	0.195187	-0.000020	0.718647
0.665450	-1.141774	0.200192	-0.000012	0.718642
0.602708	-1.278441	0.205197	-0.000001	0.718350
0.587403	-1.272511	0.210202	0.000002	0.718357
0.226305	-1.218201	0.215206	0.000070	0.718337
0.118834	-1.361807	0.220211	0.000090	0.718015
0.385725	-1.409409	0.225216	0.000040	0.718015
0.037437	-1.372736	0.230221	0.000105	0.717965
0.157322	-1.525520	0.235226	0.000083	0.717705
0.080185	-1.515648	0.240230	0.000097	0.717697
0.061042	-1.572272	0.245235	0.000101	0.717578
-0.023748	-1.658628	0.250240	0.000117	0.717378
0.293636	-1.717907	0.255245	0.000058	0.717372
0.329667	-1.835495	0.260250	0.000051	0.717152
-0.178552	-1.780995	0.265254	0.000146	0.717081
0.069458	-1.871854	0.270259	0.000100	0.716988
0.150052	-2.003507	0.275264	0.000085	0.716756
0.132318	-2.002237	0.280269	0.000088	0.716752
-0.006622	-2.119306	0.285274	0.000114	0.716471
-0.001284	-2.135227	0.290278	0.000113	0.716441
0.291843	-2.288728	0.295283	0.000059	0.716241
0.025647	-2.295006	0.300288	0.000108	0.716134
-0.160505	-2.326992	0.305293	0.000143	0.716005
-0.001600	-2.415775	0.310298	0.000114	0.715885
-0.369311	-2.409063	0.315302	0.000182	0.715768
-0.971186	-2.413493	0.320307	0.000294	0.715547
-0.918894	-2.425715	0.325312	0.000285	0.715541
-0.820892	-2.602837	0.330317	0.000267	0.715224
-0.815842	-2.597319	0.335322	0.000266	0.715237
-2.267217	-2.478470	0.340326	0.000536	0.714960
-4.966893	-2.023758	0.345331	0.001038	0.714908
-4.619742	-2.084644	0.350336	0.000974	0.714910
-4.433303	-2.128227	0.355341	0.000939	0.714889
-5.110061	-2.148247	0.360346	0.001065	0.714610
-5.316010	-2.116157	0.365350	0.001103	0.714600
-5.314390	-2.113298	0.370355	0.001103	0.714607
-5.215173	-2.130219	0.375360	0.001085	0.714608
-5.581411	-2.165378	0.380365	0.001153	0.714409
-6.450196	-2.074029	0.385370	0.001315	0.714283
-6.464082	-2.074890	0.390374	0.001317	0.714276
-6.361874	-2.093210	0.395379	0.001298	0.714275
-6.232861	-2.112729	0.400384	0.001275	0.714282
-6.765245	-2.091970	0.405389	0.001374	0.714135
-7.411853	-2.055481	0.410394	0.001494	0.713979
-7.073787	-2.120722	0.415398	0.001431	0.713968
-7.254955	-2.087111	0.420403	0.001465	0.713971
-7.309350	-2.075886	0.425408	0.001475	0.713974
-7.195911	-2.101350	0.430413	0.001454	0.713963
-7.307415	-2.218093	0.435418	0.001475	0.713692
-8.333303	-2.056106	0.440422	0.001666	0.713650
-8.401847	-2.041380	0.445427	0.001679	0.713655
-7.831177	-2.142049	0.450432	0.001573	0.713657
-8.343629	-2.054293	0.455437	0.001668	0.713650
-8.277181	-2.062553	0.460442	0.001656	0.713657
-8.500937	-2.172458	0.465446	0.001697	0.713359
-8.913464	-2.095320	0.470451	0.001774	0.713366
-9.010064	-2.078539	0.475456	0.001792	0.713365
-9.029295	-2.078129	0.480461	0.001796	0.713359
-8.850456	-2.105118	0.485466	0.001763	0.713369
-9.050740	-2.074888	0.490470	0.001800	0.713358
-9.514286	-2.154754	0.495475	0.001886	0.713035
-9.511808	-2.159229	0.500480	0.001886	0.713026
-10.182340	-2.043619	0.505485	0.002011	0.713019
-9.816200	-2.102408	0.510490	0.001943	0.713031
-9.791475	-2.109827	0.515494	0.001938	0.713025
-9.832324	-2.102781	0.520499	0.001946	0.713025
-9.952225	-2.184796	0.525504	0.001968	0.712819
-11.055594	-2.045418	0.530509	0.002174	0.712705
-10.650754	-2.113183	0.535514	0.002098	0.712714
-10.648626	-2.118496	0.540518	0.002098	0.712704
-10.922811	-2.066237	0.545523	0.002149	0.712710
-10.540715	-2.133870	0.550528	0.002078	0.712711
-10.727280	-2.118931	0.555533	0.002113	0.712675
-11.546605	-2.115507	0.560538	0.002265	0.712391
-11.502201	-2.127095	0.565542	0.002257	0.712383
-11.504143	-2.125295	0.570547	0.002258	0.712386
-11.584070	-2.109720	0.575552	0.002273	0.712389
-11.864735	-2.063319	0.580557	0.002325	0.712381
-11.603339	-2.106278	0.585562	0.002276	0.712388
-11.704836	-2.134882	0.590566	0.002295	0.712295
-12.637289	-2.073555	0.595571	0.002469	0.712086
-11.960885	-2.192095	0.600576	0.002343	0.712090
-12.325461	-2.130548	0.605581	0.002411	0.712083
-12.376808	-2.119007	0.610586	0.002420	0.712088
-12.578304	-2.084124	0.615590	0.002458	0.712086
-12.274497	-2.135893	0.620595	0.002402	0.712090
-12.754295	-2.184218	0.625600	0.002491	0.711824
-13.783755	-2.033607	0.630605	0.002683	0.711758
-13.297364	-2.115951	0.635610	0.002592	0.711767
-13.203579	-2.135120	0.640614	0.002575	0.711762
-13.499292	-2.081885	0.645619	0.002630	0.711763
-13.227023	-2.129643	0.650624	0.002579	0.711764
-13.335577	-2.113626	0.655629	0.002599	0.711757
-14.123688	-2.098738	0.660634	0.002746	0.711507
-14.634204	-2.034577	0.665638	0.002841	0.711453
-14.188830	-2.112082	0.670643	0.002758	0.711457
-14.254527	-2.097517	0.675648	0.002771	0.711463
-14.716421	-2.022615	0.680653	0.002857	0.711448
-13.989702	-2.144337	0.685658	0.002721	0.711463
-14.114828	-2.126734	0.690662	0.002745	0.711454
-14.755780	-2.106252	0.695667	0.002864	0.711267
-15.354717	-2.061284	0.700672	0.002976	0.711143
-14.809345	-2.160908	0.705677	0.002874	0.711138
-15.091465	-2.106808	0.710682	0.002927	0.711146
-15.582590	-2.023995	0.715686	0.003018	0.711136
-15.210622	-2.090027	0.720691	0.002949	0.711137
-15.132334	-2.101390	0.725696	0.002935	0.711142
-15.658677	-2.061720	0.730701	0.003033	0.711034
-16.085304	-2.065291	0.735706	0.003112	0.710875
-15.735483	-2.132186	0.740710	0.003047	0.710866
-16.407151	-2.009268	0.745715	0.003172	0.710872
-16.107032	-2.060937	0.750720	0.003116	0.710875
-15.908595	-2.100626	0.755725	0.003079	0.710867
-16.100756	-2.061420	0.760730	0.003115	0.710877
-16.245278	-2.076000	0.765734	0.003142	0.710796
-16.695810	-2.126814	0.770739	0.003226	0.710534
-16.584857	-2.142593	0.775744	0.003206	0.710542
-17.359300	-2.008668	0.780749	0.003350	0.710534
-16.878103	-2.090922	0.785754	0.003260	0.710541
-16.757706	-2.115962	0.790758	0.003238	0.710533
-17.141813	-2.045919	0.795763	0.003309	0.710536
-16.888903	-2.151249	0.800768	0.003262	0.710416
-17.949305	-2.062752	0.805773	0.003460	0.710215
-17.588650	-2.121462	0.810778	0.003393	0.710226
-18.107147	-2.032862	0.815782	0.003489	0.710218
-18.182081	-2.018998	0.820787	0.003503	0.710219
-17.625446	-2.117899	0.825792	0.003400	0.710220
-18.102516	-2.037031	0.830797	0.003489	0.710211
-17.865688	-2.102182	0.835802	0.003445	0.710166
-18.421052	-2.140085	0.840806	0.003548	0.709892
-18.781919	-2.074181	0.845811	0.003615	0.709895
-18.937514	-2.043448	0.850816	0.003644	0.709901
-18.881209	-2.058939	0.855821	0.003634	0.709890
-18.685176	-2.090897	0.860826	0.003597	0.709896
-19.082098	-2.022394	0.865830	0.003671	0.709891
-18.885364	-2.055531	0.870835	0.003635	0.709895
-18.854086	-2.186826	0.875840	0.003629	0.709643
-19.982295	-2.010684	0.880845	0.003839	0.709593
-19.806505	-2.036697	0.885850	0.003806	0.709604
-19.685870	-2.063649	0.890854	0.003784	0.709593
-19.734427	-2.054641	0.895859	0.003793	0.709594
-19.773627	-2.045311	0.900864	0.003800	0.709598
-19.837928	-2.037633	0.905869	0.003812	0.709591
-19.902770	-2.131972	0.910874	0.003825	0.709379
-20.926354	-2.007915	0.915878	0.004015	0.709262
-20.680178	-2.051854	0.920883	0.003969	0.709262
-20.555089	-2.072306	0.925888	0.003946	0.709265
-21.016200	-1.993373	0.930893	0.004032	0.709259
-20.491695	-2.081838	0.935898	0.003934	0.709268
-20.687793	-2.050010	0.940902	0.003971	0.709262
-20.863320	-2.046880	0.945907	0.004004	0.709206
-21.506032	-2.054947	0.950912	0.004123	0.708960
-21.414757	-2.077599	0.955917	0.004106	0.708947
-21.495217	-2.058385	0.960922	0.004121	0.708957
-21.706426	-2.023512	0.965926	0.004161	0.708951
-21.766953	-2.011786	0.970931	0.004172	0.708953
-21.446136	-2.065713	0.975936	0.004112	0.708960
-21.687640	-2.027079	0.980941	0.004157	0.708951
-21.749715	-2.144563	0.985946	0.004169	0.708693
-22.483468	-2.042714	0.990950	0.004306	0.708635
-22.233198	-2.087930	0.995955	0.004259	0.708634
-22.172314	-2.096242	1.000960	0.004248	0.708639
-22.639727	-2.016024	1.005965	0.004335	0.708633
-22.158557	-2.098178	1.010970	0.004245	0.708640
-22.407464	-2.064609	1.015974	0.004292	0.708618
-23.195677	-2.060695	1.020979	0.004439	0.708344
-22.915094	-2.106484	1.025984	0.004386	0.708353
-23.383617	-2.029142	1.030989	0.004474	0.708340
-23.146476	-2.066644	1.035994	0.004430	0.708350
-23.040693	-2.085880	1.040998	0.004410	0.708349
-23.319482	-2.037441	1.046003	0.004462	0.708346
-23.184738	-2.091468	1.051008	0.004437	0.708286
-24.205134	-2.049455	1.056013	0.004627	0.708005
-23.760674	-2.123984	1.061018	0.004544	0.708015
-24.374524	-2.019104	1.066022	0.004659	0.708006
-24.304752	-2.030249	1.071027	0.004646	0.708008
-23.952908	-2.090219	1.076032	0.004580	0.708014
-24.348531	-2.024383	1.081037	0.004654	0.708004
-24.309703	-2.027951	1.086042	0.004647	0.708011
-24.614259	-2.128732	1.091046	0.004703	0.707700
-25.141316	-2.038459	1.096051	0.004802	0.707692
-25.189690	-2.024893	1.101056	0.004811	0.707702
-24.999501	-2.063061	1.106061	0.004775	0.707693
-24.854377	-2.085028	1.111066	0.004748	0.707701
-25.339779	-2.001049	1.116070	0.004839	0.707696
-25.166493	-2.031147	1.121075	0.004806	0.707697
-24.897981	-2.201163	1.126080	0.004757	0.707452
-26.148155	-2.020865	1.131085	0.004989	0.707367
-26.219442	-2.002946	1.136090	0.005003	0.707377
-25.954495	-2.053307	1.141094	0.004953	0.707371
-26.041100	-2.037752	1.146099	0.004970	0.707371
-25.812006	-2.075774	1.151104	0.004927	0.707376
-25.966716	-2.051776	1.156109	0.004956	0.707369
-25.930322	-2.167462	1.161114	0.004949	0.707150
-26.997670	-2.012532	1.166118	0.005148	0.707079
-27.165521	-1.984091	1.171123	0.005179	0.707076
-26.560723	-2.089771	1.176128	0.005067	0.707080
-26.941226	-2.026852	1.181133	0.005137	0.707070
-26.735729	-2.057834	1.186138	0.005099	0.707081
-26.630545	-2.078712	1.191142	0.005080	0.707077
-27.175863	-2.113642	1.196147	0.005181	0.706812
-27.875183	-2.018919	1.201152	0.005312	0.706751
-27.883938	-2.023220	1.206157	0.005313	0.706740
-27.514283	-2.083967	1.211162	0.005245	0.706750
-27.993406	-2.000438	1.216166	0.005334	0.706746
-28.174489	-1.969559	1.221171	0.005367	0.706743
-27.660058	-2.055913	1.226176	0.005272	0.706754
-27.671803	-2.111654	1.231181	0.005274	0.706637
-28.660809	-2.032280	1.236186	0.005458	0.706443
-28.262100	-2.106441	1.241190	0.005384	0.706436
-28.588127	-2.048680	1.246195	0.005445	0.706435
-28.344819	-2.088466	1.251200	0.005400	0.706443
-28.696710	-2.030017	1.256205	0.005465	0.706434
-28.390034	-2.079194	1.261210	0.005408	0.706445
-28.641564	-2.145667	1.266214	0.005455	0.706221
-29.958733	-1.957097	1.271219	0.005700	0.706128
-29.647839	-2.011880	1.276224	0.005642	0.706129
-29.422409	-2.055197	1.281229	0.005600	0.706123
-29.579919	-2.024480	1.286234	0.005630	0.706128
-29.587662	-2.024260	1.291238	0.005631	0.706126
-29.449966	-2.049805	1.296243	0.005606	0.706123
-29.442057	-2.101428	1.301248	0.005604	0.706022
-30.756754	-1.951185	1.306253	0.005849	0.705853
-30.071275	-2.068970	1.311258	0.005722	0.705862
-30.222295	-2.043872	1.316262	0.005750	0.705858
-30.822471	-1.935889	1.321267	0.005861	0.705860
-30.234903	-2.039403	1.326272	0.005752	0.705862
-30.226349	-2.046122	1.331277	0.005751	0.705852
-30.247455	-2.104073	1.336282	0.005755	0.705728
-31.478524	-1.986493	1.341286	0.005984	0.705523
-31.293008	-2.018002	1.346291	0.005949	0.705526
-31.254011	-2.021303	1.351296	0.005942	0.705533
-31.609107	-1.962157	1.356301	0.006008	0.705525
-31.261358	-2.020914	1.361306	0.005944	0.705531
-31.095883	-2.051876	1.366310	0.005913	0.705528
-31.459345	-2.005159	1.371315	0.005980	0.705491
-31.836916	-2.075246	1.376320	0.006051	0.705215
-32.129193	-2.027138	1.381325	0.006105	0.705207
-32.384308	-1.979724	1.386330	0.006153	0.705210
-32.241020	-2.004096	1.391334	0.006126	0.705213
-32.355228	-1.982572	1.396339	0.006148	0.705215
-32.061982	-2.032664	1.401344	0.006093	0.705219
-32.361478	-1.986138	1.406349	0.006149	0.705205
-32.518400	-2.095493	1.411354	0.006178	0.704929
-32.952502	-2.037755	1.416358	0.006259	0.704889
-33.060664	-2.020485	1.421363	0.006279	0.704885
-32.835150	-2.057732	1.426368	0.006237	0.704891
-32.797336	-2.066985	1.431373	0.006230	0.704886
-32.912885	-2.043479	1.436378	0.006252	0.704891
-33.084418	-2.045362	1.441382	0.006284	0.704826
-34.040227	-1.992649	1.446387	0.006462	0.704589
-33.532618	-2.079561	1.451392	0.006367	0.704596
-34.130640	-1.978731	1.456397	0.006479	0.704584
-33.948632	-2.006521	1.461402	0.006445	0.704593
-33.798053	-2.033937	1.466406	0.006417	0.704592
-34.124928	-1.979192	1.471411	0.006478	0.704585
-33.765765	-2.057184	1.476416	0.006411	0.704557
-34.685867	-2.043182	1.481421	0.006582	0.704254
-34.683362	-2.041108	1.486426	0.006582	0.704259
-34.895469	-2.003372	1.491430	0.006621	0.704259
-34.822151	-2.016978	1.496435	0.006608	0.704258
-34.570484	-2.057962	1.501440	0.006561	0.704265
-35.088027	-1.971627	1.506445	0.006657	0.704253
-34.914363	-1.999404	1.511450	0.006625	0.704260
-35.291941	-2.074842	1.516454	0.006695	0.703972
-35.997220	-1.961575	1.521459	0.006827	0.703947
-35.862533	-1.981710	1.526464	0.006802	0.703954
-35.696782	-2.015738	1.531469	0.006771	0.703945
-35.675693	-2.016513	1.536474	0.006767	0.703951
-35.854874	-1.983640	1.541478	0.006800	0.703953
-36.106942	-1.941605	1.546483	0.006847	0.703947
-35.617473	-2.106018	1.551488	0.006756	0.703791
-36.823325	-1.973588	1.556493	0.006981	0.703625
-36.405192	-2.045218	1.561498	0.006903	0.703630
-36.404907	-2.043330	1.566502	0.006903	0.703634
-36.610150	-2.009175	1.571507	0.006941	0.703629
-36.305908	-2.059962	1.576512	0.006885	0.703636
-36.526590	-2.025220	1.581517	0.006926	0.703627
-36.820242	-2.085836	1.586522	0.006981	0.703399
-37.361770	-2.017939	1.591526	0.007082	0.703341
-37.698445	-1.960082	1.596531	0.007144	0.703336
-37.251768	-2.035412	1.601536	0.007061	0.703345
-37.659100	-1.967008	1.606541	0.007137	0.703336
-37.552633	-1.986021	1.611546	0.007117	0.703336
-37.132693	-2.061107	1.616550	0.007039	0.703335
-37.764526	-2.095231	1.621555	0.007157	0.703039
-38.303881	-2.015960	1.626560	0.007257	0.703005
-38.567719	-1.974446	1.631565	0.007306	0.702994
-38.224125	-2.031404	1.636570	0.007243	0.703002
-38.526945	-1.975330	1.641574	0.007299	0.703006
-38.688885	-1.951711	1.646579	0.007329	0.702996
-38.071197	-2.057337	1.651584	0.007214	0.703005
-38.830773	-2.036485	1.656589	0.007356	0.702773
-39.332804	-1.989190	1.661594	0.007449	0.702688
-38.774375	-2.087192	1.666598	0.007345	0.702691
-39.196450	-2.013256	1.671603	0.007424	0.702688
-39.396541	-1.973604	1.676608	0.007461	0.702696
-39.302588	-1.994981	1.681613	0.007444	0.702686
-39.040048	-2.037184	1.686618	0.007395	0.702696
-39.463556	-2.083522	1.691622	0.007474	0.702449
-40.287764	-1.975373	1.696627	0.007627	0.702371
-39.874427	-2.046469	1.701632	0.007550	0.702376
-40.117359	-2.008791	1.706637	0.007596	0.702364
-40.183382	-1.991882	1.711642	0.007608	0.702375
-39.793217	-2.063826	1.716646	0.007535	0.702370
-39.900509	-2.047241	1.721651	0.007555	0.702364
-40.627605	-2.052627	1.726656	0.007691	0.702091
-41.091260	-1.982540	1.731661	0.007777	0.702066
-40.771455	-2.035536	1.736666	0.007718	0.702074
-40.550117	-2.077267	1.741670	0.007677	0.702069
-41.087594	-1.984026	1.746675	0.007777	0.702064
-40.671892	-2.051728	1.751680	0.007699	0.702077
-40.943551	-2.034346	1.756685	0.007750	0.702014
-41.925651	-1.995198	1.761690	0.007933	0.701739
-41.760943	-2.023979	1.766694	0.007902	0.701740
-42.047171	-1.974795	1.771699	0.007956	0.701736
-41.917774	-1.993772	1.776704	0.007932	0.701744
-41.748075	-2.028147	1.781709	0.007900	0.701736
-41.609699	-2.050691	1.786714	0.007874	0.701740
-41.608778	-2.057405	1.791718	0.007874	0.701727
-42.749693	-2.000403	1.796723	0.008087	0.701430
-42.493619	-2.042198	1.801728	0.008039	0.701438
-42.573867	-2.032935	1.806733	0.008054	0.701427
-42.746945	-2.000724	1.811738	0.008086	0.701430
-42.693316	-2.009393	1.816742	0.008076	0.701432
-42.612105	-2.028068	1.821747	0.008061	0.701423
-42.554325	-2.044068	1.826752	0.008051	0.701412
-43.544743	-2.014326	1.831757	0.008235	0.701114
-43.394441	-2.038190	1.836762	0.008207	0.701120
-43.369029	-2.042908	1.841766	0.008202	0.701119
-43.622846	-2.000655	1.846771	0.008250	0.701113
-43.352156	-2.041591	1.851776	0.008199	0.701128
-43.523689	-2.016474	1.856781	0.008231	0.701117
-43.484206	-2.048046	1.861786	0.008224	0.701067
-44.190163	-2.020078	1.866790	0.008356	0.700869
-43.889115	-2.076173	1.871795	0.008300	0.700864
-43.733517	-2.099558	1.876800	0.008271	0.700872
-44.594183	-1.949299	1.881805	0.008431	0.700866
-44.207867	-2.016323	1.886810	0.008359	0.700869
-44.089445	-2.034004	1.891814	0.008337	0.700876
-44.925094	-2.032772	1.896819	0.008493	0.700577
-45.288303	-1.988523	1.901824	0.008560	0.700535
-45.064863	-2.032821	1.906829	0.008519	0.700526
-45.017097	-2.039331	1.911834	0.008510	0.700530
-45.398566	-1.970695	1.916838	0.008581	0.700531
-45.297281	-1.991020	1.921843	0.008562	0.700526
-44.951458	-2.045976	1.926848	0.008498	0.700540
-45.802922	-2.037922	1.931853	0.008656	0.700248
-46.200524	-1.981952	1.936858	0.008730	0.700218
-45.900380	-2.036270	1.941862	0.008675	0.700216
-46.215231	-1.981088	1.946867	0.008733	0.700214
-46.062502	-2.006391	1.951872	0.008705	0.700218
-45.985909	-2.023043	1.956877	0.008691	0.700212
-46.123482	-1.996123	1.961882	0.008716	0.700216
-46.540786	-2.054064	1.966886	0.008794	0.699948
-46.873614	-2.023862	1.971891	0.008856	0.699889
-46.859597	-2.023241	1.976896	0.008854	0.699895
-47.015832	-1.997840	1.981901	0.008883	0.699890
-47.142315	-1.976974	1.986906	0.008906	0.699886
-47.032064	-1.991551	1.991910	0.008886	0.699896
-47.063468	-1.991291	1.996915	0.008892	0.699886
-47.425968	-2.047727	2.001920	0.008959	0.699640

-47.610722	-2.036288	2.011917	0.008994	0.699596
-47.949362	-1.973163	2.021914	0.009057	0.699601
-47.915552	-1.980412	2.031910	0.009051	0.699599
-47.480270	-2.060441	2.041907	0.008970	0.699593
-47.709601	-2.018153	2.051904	0.009013	0.699596
-47.625734	-2.032904	2.061901	0.008997	0.699596
-47.440326	-2.067378	2.071898	0.008963	0.699593
-47.564594	-2.045055	2.081894	0.008986	0.699593
-47.436641	-2.068322	2.091891	0.008962	0.699592
-47.832708	-1.994264	2.101888	0.009036	0.699599
-47.684061	-2.022183	2.111885	0.009008	0.699596
-47.704184	-2.019931	2.121882	0.009012	0.699593
-47.780825	-1.996557	2.131878	0.009026	0.699613
-46.864429	-2.022986	2.141875	0.008856	0.699891
-46.886538	-2.019149	2.151872	0.008860	0.699890
-46.769305	-2.040889	2.161869	0.008838	0.699888
-46.765635	-2.040802	2.171866	0.008838	0.699890
-46.737370	-2.039517	2.181862	0.008833	0.699902
-46.122864	-1.998112	2.191859	0.008718	0.700209
-45.973051	-2.023773	2.201856	0.008691	0.700211
-45.958380	-2.024684	2.211853	0.008688	0.700214
-45.929369	-2.030270	2.221850	0.008683	0.700213
-45.344954	-1.990210	2.231846	0.008574	0.700505
-44.946707	-2.050916	2.241843	0.008500	0.700526
-44.840322	-2.068641	2.251840	0.008480	0.700528
-44.920900	-2.054148	2.261837	0.008495	0.700528
-44.366314	-2.009239	2.271834	0.008392	0.700820
-44.224787	-2.011367	2.281830	0.008366	0.700866
-43.974056	-2.055096	2.291827	0.008319	0.700868
-44.132444	-2.019944	2.301824	0.008349	0.700882
-43.328347	-2.046290	2.311821	0.008199	0.701119
-43.317692	-2.048063	2.321818	0.008197	0.701119
-43.489112	-2.018224	2.331814	0.008229	0.701117
-43.128184	-1.997269	2.341811	0.008162	0.701290
-42.703749	-2.002433	2.351808	0.008083	0.701433
-42.502599	-2.035970	2.361805	0.008046	0.701437
-42.518676	-2.003686	2.371802	0.008049	0.701497
-41.777432	-2.014504	2.381798	0.007911	0.701742
-41.691654	-2.031756	2.391795	0.007895	0.701738
-41.774971	-2.014305	2.401792	0.007911	0.701743
-41.088707	-2.006739	2.411789	0.007783	0.702006
-40.930287	-2.003299	2.421786	0.007754	0.702070
-40.805864	-2.026823	2.431782	0.007731	0.702067
-40.614348	-2.015296	2.441779	0.007695	0.702159
-40.174675	-1.988689	2.451776	0.007613	0.702371
-40.016273	-2.017691	2.461773	0.007584	0.702369
-40.288262	-1.959106	2.471770	0.007634	0.702390
-39.171475	-2.009370	2.481766	0.007427	0.702690
-39.309193	-1.985505	2.491763	0.007452	0.702689
-39.048342	-2.030141	2.501760	0.007404	0.702692
-38.757490	-1.980901	2.511757	0.007350	0.702897
-38.369484	-1.995640	2.521754	0.007278	0.703006
-38.163230	-2.033520	2.531750	0.007239	0.703004
-38.254317	-1.985321	2.541747	0.007256	0.703068
-37.281797	-2.022130	2.551744	0.007075	0.703344
-37.189046	-2.037957	2.561741	0.007058	0.703345
-37.571861	-1.967268	2.571738	0.007130	0.703350
-37.045623	-1.965965	2.581734	0.007032	0.703542
-36.753254	-1.968828	2.591731	0.006977	0.703641
-36.701978	-1.976797	2.601728	0.006968	0.703643
-36.244098	-2.000442	2.611725	0.006883	0.703760
-35.813521	-1.980322	2.621722	0.006803	0.703955
-35.655568	-2.010327	2.631718	0.006773	0.703952
-35.784942	-1.988727	2.641715	0.006798	0.703948
-34.981678	-1.994286	2.651712	0.006648	0.704226
-34.920679	-1.986316	2.661709	0.006637	0.704264
-34.628081	-2.039779	2.671706	0.006582	0.704261
-34.664219	-1.975503	2.681702	0.006589	0.704377
-33.691391	-2.043260	2.691699	0.006408	0.704590
-33.740535	-2.032979	2.701696	0.006417	0.704593
-33.931562	-1.999694	2.711693	0.006453	0.704591
-33.285775	-2.013505	2.721690	0.006333	0.704795
-33.132925	-1.996329	2.731686	0.006305	0.704885
-33.231488	-1.976307	2.741683	0.006323	0.704889
-32.857487	-1.995323	2.751680	0.006253	0.704985
-32.003997	-2.032509	2.761677	0.006095	0.705216
-32.014800	-2.032437	2.771674	0.006097	0.705213
-32.096900	-2.017677	2.781670	0.006112	0.705213
-31.525839	-2.025679	2.791667	0.006006	0.705401
-30.946629	-2.066322	2.801664	0.005898	0.705527
-31.310524	-1.998620	2.811661	0.005966	0.705533
-31.296588	-1.993639	2.821658	0.005963	0.705547
-30.687221	-1.940912	2.831654	0.005850	0.705872
-30.516829	-1.973951	2.841651	0.005818	0.705866
-30.127289	-2.045584	2.851648	0.005746	0.705862
-29.958220	-1.986584	2.861645	0.005715	0.706041
-29.665204	-1.991662	2.871642	0.005660	0.706136
-29.694405	-1.985982	2.881638	0.005666	0.706136
-29.551172	-1.965058	2.891635	0.005639	0.706230
-28.705858	-2.002622	2.901632	0.005482	0.706457
-28.753119	-1.995278	2.911629	0.005491	0.706454
-28.882379	-1.971687	2.921626	0.005515	0.706455
-28.271282	-1.926241	2.931622	0.005401	0.706765
-28.060875	-1.963496	2.941619	0.005362	0.706766
-27.823593	-2.010287	2.951616	0.005318	0.706756
-27.262368	-1.985726	2.961613	0.005214	0.707007
-26.962807	-1.998205	2.971610	0.005158	0.707089
-27.025695	-1.990296	2.981606	0.005170	0.707082
-26.921019	-1.978897	2.991603	0.005150	0.707142
-26.161205	-1.993625	3.001600	0.005009	0.707384
-26.110770	-1.999995	3.011597	0.005000	0.707389
-26.165044	-1.991170	3.021594	0.005010	0.707387
-25.722418	-1.945509	3.031590	0.004927	0.707637
-25.179193	-2.009472	3.041587	0.004826	0.707703
-25.101818	-2.019629	3.051584	0.004812	0.707710
-25.251220	-1.961443	3.061581	0.004840	0.707773
-24.209472	-2.025242	3.071578	0.004646	0.708017
-24.417476	-1.989529	3.081574	0.004685	0.708014
-24.322492	-2.007537	3.091571	0.004667	0.708012
-23.834381	-1.985885	3.101568	0.004577	0.708230
-23.431334	-1.995166	3.111565	0.004502	0.708355
-23.214982	-2.035270	3.121562	0.004461	0.708352
-23.401555	-2.000610	3.131558	0.004496	0.708354
-22.394805	-2.037582	3.141555	0.004309	0.708639
-22.378708	-2.039076	3.151552	0.004306	0.708642
-22.267115	-2.059303	3.161549	0.004285	0.708641
-22.354749	-2.014773	3.171546	0.004302	0.708699
-21.524299	-2.036331	3.181542	0.004147	0.708952
-21.209925	-2.091404	3.191539	0.004089	0.708954
-21.476890	-2.041482	3.201536	0.004138	0.708958
-21.343657	-2.003082	3.211533	0.004114	0.709082
-20.640656	-2.037111	3.221530	0.003983	0.709265
-20.830422	-2.003444	3.231526	0.004018	0.709264
-20.524154	-2.058633	3.241523	0.003961	0.709263
-20.050526	-1.982909	3.251520	0.003873	0.709583
-19.478585	-2.080044	3.261517	0.003767	0.709593
-19.599863	-2.055808	3.271514	0.003790	0.709598
-19.675593	-2.002461	3.281510	0.003804	0.709677
-18.658459	-2.076629	3.291507	0.003615	0.709891
-18.888985	-2.033981	3.301504	0.003658	0.709894
-18.787445	-2.051478	3.311501	0.003639	0.709895
-18.070612	-2.063384	3.321498	0.003505	0.710127
-17.929112	-2.044020	3.331494	0.003479	0.710216
-17.669675	-2.088594	3.341491	0.003431	0.710219
-17.799257	-2.063933	3.351488	0.003455	0.710222
-17.030352	-2.058618	3.361485	0.003312	0.710506
-17.096785	-2.032534	3.371482	0.003324	0.710534
-16.925318	-2.063897	3.381478	0.003293	0.710532
-16.762191	-2.047615	3.391475	0.003262	0.710623
-15.966694	-2.062761	3.401472	0.003114	0.710876
-15.823642	-2.088709	3.411469	0.003088	0.710874
-16.071522	-2.044575	3.421466	0.003134	0.710874
-15.760302	-2.021071	3.431462	0.003076	0.711032
-15.267392	-2.053645	3.441459	0.002984	0.711142
-15.092700	-2.084094	3.451456	0.002952	0.711143
-15.071251	-2.074791	3.461453	0.002948	0.711169
-14.597097	-2.013269	3.471450	0.002860	0.711460
-14.176679	-2.089101	3.481446	0.002782	0.711458
-14.339725	-2.060749	3.491443	0.002812	0.711457
-14.073155	-2.010689	3.501440	0.002763	0.711651
-13.305040	-2.088672	3.511437	0.002620	0.711768
-13.719012	-2.013932	3.521434	0.002697	0.711770
-13.401271	-2.033144	3.531430	0.002638	0.711844
-12.754567	-2.022091	3.541427	0.002517	0.712096
-12.479943	-2.070576	3.551424	0.002466	0.712097
-12.565039	-2.052388	3.561421	0.002482	0.712103
-12.003100	-2.035950	3.571418	0.002378	0.712335
-11.651858	-2.070785	3.581414	0.002313	0.712390
-11.788860	-2.045781	3.591411	0.002338	0.712391
-11.694724	-2.018062	3.601408	0.002321	0.712479
-10.866466	-2.046527	3.611405	0.002167	0.712716
-10.730922	-2.072392	3.621402	0.002141	0.712713
-10.657211	-2.085357	3.631398	0.002128	0.712713
-10.207266	-2.058515	3.641395	0.002044	0.712926
-9.863891	-2.068014	3.651392	0.001980	0.713028
-9.899504	-2.061033	3.661389	0.001987	0.713029
-10.045553	-2.014749	3.671386	0.002014	0.713070
-9.112108	-2.029164	3.681382	0.001841	0.713372
-9.337020	-1.988069	3.691379	0.001882	0.713374
-8.929987	-2.060685	3.701376	0.001807	0.713373
-8.574951	-2.019737	3.711373	0.001741	0.713580
-8.134842	-2.056278	3.721370	0.001659	0.713663
-8.063417	-2.069504	3.731366	0.001646	0.713662
-8.393476	-1.982171	3.741363	0.001707	0.713719
-7.317349	-2.043631	3.751360	0.001507	0.713978
-7.251096	-2.052947	3.761357	0.001495	0.713982
-7.297375	-2.042375	3.771354	0.001503	0.713987
-6.610385	-2.062623	3.781350	0.001376	0.714190
-6.373625	-2.057160	3.791347	0.001332	0.714284
-6.041918	-2.116865	3.801344	0.001270	0.714283
-6.357248	-2.060610	3.811341	0.001329	0.714283
-5.796713	-2.009379	3.821338	0.001224	0.714583
-5.178631	-2.103645	3.831334	0.001110	0.714614
-5.589855	-2.025745	3.841331	0.001186	0.714623
-5.394380	-2.002507	3.851328	0.001150	0.714738
-4.427725	-2.084732	3.861325	0.000970	0.714916
-4.517797	-2.069625	3.871322	0.000987	0.714914
-4.447647	-2.083056	3.881318	0.000974	0.714912
-3.812085	-2.086947	3.891315	0.000856	0.715129
-3.763531	-2.039307	3.901312	0.000847	0.715241
-3.641320	-2.061775	3.911309	0.000824	0.715239
-3.666578	-2.034580	3.921306	0.000829	0.715284
-2.782938	-2.056430	3.931302	0.000664	0.715553
-2.679137	-2.075225	3.941299	0.000645	0.715552
-2.591193	-2.091826	3.951296	0.000629	0.715550
-2.323378	-2.061368	3.961293	0.000579	0.715705
-1.869438	-2.051900	3.971290	0.000495	0.715884
-2.131534	-2.006552	3.981286	0.000543	0.715881
-1.729868	-2.077293	3.991283	0.000469	0.715882
-2.394141	-1.831260	4.001280	0.000592	0.716135
-1.862988	-1.924352	4.011277	0.000494	0.716138
-1.318674	-1.956364	4.021274	0.000392	0.716266
-2.159295	-1.712159	4.031270	0.000549	0.716453
-0.883603	-1.938874	4.041267	0.000312	0.716454
-1.210846	-1.726594	4.051264	0.000373	0.716759
-1.165125	-1.734649	4.061261	0.000364	0.716759
-0.924072	-1.656526	4.071258	0.000319	0.716998
-1.622364	-1.487300	4.081254	0.000449	0.717087
-0.642711	-1.534651	4.091251	0.000267	0.717338
-1.139037	-1.423933	4.101248	0.000359	0.717382
-1.208482	-1.249977	4.111245	0.000372	0.717702
-0.312158	-1.360256	4.121242	0.000206	0.717799
-0.701069	-1.181474	4.131238	0.000278	0.718015
-0.117406	-1.175100	4.141235	0.000169	0.718233
-0.554929	-1.027122	4.151232	0.000251	0.718372
-0.466527	-0.901828	4.161229	0.000234	0.718650
-0.513572	-0.797137	4.171226	0.000243	0.718840
-0.619575	-0.667311	4.181222	0.000263	0.719059
-0.047597	-0.661422	4.191219	0.000156	0.719271
0.002405	-0.506483	4.201216	0.000147	0.719594
-0.099693	-0.381517	4.211213	0.000166	0.719804
0.039317	-0.283826	4.221210	0.000140	0.720046
0.254054	-0.195570	4.231206	0.000100	0.720295
0.151100	-0.040546	4.241203	0.000120	0.720564
0.000000	0.180918	4.251200	0.000148	0.720947

0.230083	0.714282	4.256205	0.000104	0.722076
0.299123	1.977109	4.261210	0.000091	0.724578
0.845482	3.729647	4.266214	-0.000012	0.728191
1.651957	6.004766	4.271219	-0.000164	0.732889
2.302759	8.824847	4.276224	-0.000287	0.738551
2.994966	12.112214	4.281229	-0.000418	0.745074
3.826182	15.848652	4.286234	-0.000575	0.752435
4.538430	20.006413	4.291238	-0.000710	0.760471
5.313207	24.555363	4.296243	-0.000857	0.769165
6.172777	29.471535	4.301248	-0.001020	0.778458
6.537966	34.809015	4.306253	-0.001092	0.788242
7.067425	40.444213	4.311258	-0.001194	0.798488
7.986116	46.309698	4.316262	-0.001369	0.809127
8.460199	52.538895	4.321267	-0.001461	0.820122
9.150607	59.010759	4.326272	-0.001594	0.831450
9.687514	65.718868	4.331277	-0.001698	0.842978
10.290364	72.649937	4.336282	-0.001815	0.854739
10.964096	79.764749	4.341286	-0.001945	0.866661
11.655441	87.065618	4.346291	-0.002078	0.878727
12.503934	94.519399	4.351296	-0.002241	0.890916
13.032146	102.181166	4.356301	-0.002344	0.903179
14.091509	109.907459	4.361306	-0.002547	0.915521
15.027235	117.767910	4.366310	-0.002726	0.927871
15.432742	125.843491	4.371315	-0.002807	0.940242
15.979263	134.002139	4.376320	-0.002914	0.952613
16.584323	142.219030	4.381325	-0.003032	0.964926
17.209403	150.527254	4.386330	-0.003154	0.977220
17.993400	158.894121	4.391334	-0.003305	0.989486
18.710125	167.306436	4.396339	-0.003444	1.001648
19.667683	175.739571	4.401344	-0.003628	1.013752
20.410211	184.239596	4.406349	-0.003771	1.025753
21.662208	192.710390	4.411354	-0.004010	1.037696
22.544768	201.257506	4.416358	-0.004180	1.049518
23.265382	209.858901	4.421363	-0.004319	1.061244
23.741752	218.541095	4.426368	-0.004414	1.072892
24.313695	227.172169	4.431373	-0.004526	1.084370
25.215754	235.786467	4.436378	-0.004699	1.095779
25.654291	244.470243	4.441382	-0.004787	1.107056
26.335857	253.116295	4.446387	-0.004919	1.118225
27.460232	261.699492	4.451392	-0.005134	1.129299
28.358803	270.316537	4.456397	-0.005307	1.140259
28.810879	279.030923	4.461402	-0.005397	1.151141
29.640657	287.641268	4.466406	-0.005557	1.161871
30.204931	296.281766	4.471411	-0.005667	1.172485
30.842602	304.903555	4.476416	-0.005792	1.182996
31.228687	313.555532	4.481421	-0.005869	1.193399
31.930462	322.132380	4.486426	-0.006005	1.203686
32.805893	330.685852	4.491430	-0.006174	1.213894
33.607309	339.223122	4.496435	-0.006329	1.223982
34.413005	347.795796	4.501440	-0.006484	1.234029
35.115779	356.314512	4.506445	-0.006621	1.243913
35.600087	364.885327	4.511450	-0.006716	1.253736
36.084797	373.423557	4.516454	-0.006812	1.263446
36.646084	381.945363	4.521459	-0.006922	1.273077
37.596893	390.387740	4.526464	-0.007105	1.282621
38.130764	398.890705	4.531469	-0.007210	1.292083
38.773023	407.362828	4.536474	-0.007335	1.301463
39.720858	415.846673	4.541478	-0.007517	1.310843
40.250832	424.361473	4.546483	-0.007621	1.320114
40.771280	432.797622	4.551488	-0.007723	1.329235
41.575091	441.174430	4.556493	-0.007878	1.338280
41.921576	449.619779	4.561498	-0.007948	1.347257
42.979222	457.950154	4.566502	-0.008151	1.356177
43.649823	466.319794	4.571507	-0.008281	1.365013
44.490469	474.691855	4.576512	-0.008443	1.373823
44.851460	483.101875	4.581517	-0.008515	1.382534
45.682423	491.461569	4.586522	-0.008676	1.391218
46.288854	499.836180	4.591526	-0.008794	1.399826
46.941861	508.166892	4.596531	-0.008921	1.408344
47.954818	516.464614	4.601536	-0.009115	1.416837
48.542927	524.797772	4.606541	-0.009230	1.425245
49.002273	533.168976	4.611546	-0.009321	1.433620
49.726037	541.461828	4.616550	-0.009461	1.441911
50.535397	549.748372	4.621555	-0.009617	1.450163
51.105604	558.090463	4.626560	-0.009728	1.458383
51.598951	566.406506	4.631565	-0.009826	1.466520
52.581211	574.710485	4.636570	-0.010014	1.474677
53.373792	582.973475	4.641574	-0.010167	1.482720
53.654299	591.304075	4.646579	-0.010224	1.490704
54.342433	599.581212	4.651584	-0.010358	1.498657
55.229833	607.788475	4.656589	-0.010528	1.506534
55.918102	616.070149	4.661594	-0.010662	1.514408
56.979510	624.267434	4.666598	-0.010865	1.522219
57.759561	632.518361	4.671603	-0.011015	1.529997
58.729934	640.762296	4.676608	-0.011201	1.537758
59.063486	649.058337	4.681613	-0.011269	1.545432
59.648068	657.360605	4.686618	-0.011383	1.553111
60.025021	665.637016	4.691622	-0.011459	1.560698
60.633672	673.855309	4.696627	-0.011577	1.568230
61.262036	682.102038	4.701632	-0.011700	1.575753
61.740860	690.340323	4.706637	-0.011794	1.583212
62.160769	698.599336	4.711642	-0.011878	1.590645
62.637872	706.839046	4.716646	-0.011972	1.598035
63.079354	715.046450	4.721651	-0.012059	1.605357
63.784382	723.262993	4.726656	-0.012196	1.612691
64.123439	731.496205	4.731661	-0.012264	1.619955
64.504605	739.733543	4.736666	-0.012341	1.627195
65.247806	747.965403	4.741670	-0.012484	1.634449
65.641383	756.161645	4.746675	-0.012563	1.641591
66.502509	764.302925	4.751680	-0.012729	1.648720
66.956506	772.515055	4.756685	-0.012818	1.655822
67.700631	780.661579	4.761690	-0.012962	1.662877
68.088481	788.886070	4.766694	-0.013040	1.669921
68.634467	797.072102	4.771699	-0.013147	1.676923
69.467003	805.209795	4.776704	-0.013307	1.683893
70.007803	813.395245	4.781709	-0.013413	1.690836
70.509256	821.606384	4.786714	-0.013512	1.697767
71.159333	829.777877	4.791718	-0.013638	1.704656
71.365257	838.020604	4.796723	-0.013682	1.711517
71.784506	846.235299	4.801728	-0.013765	1.718356
72.108232	854.384111	4.806733	-0.013831	1.725101
72.829754	862.540042	4.811738	-0.013970	1.731877
73.384182	870.696215	4.816742	-0.014079	1.738605
73.895252	878.827882	4.821747	-0.014179	1.745281
74.611195	886.992842	4.826752	-0.014318	1.751985
74.888279	895.185398	4.831757	-0.014375	1.758630
75.482517	903.311012	4.836762	-0.014490	1.765236
76.296374	911.448752	4.841766	-0.014647	1.771853
76.537027	919.637814	4.846771	-0.014697	1.778416
76.749630	927.847192	4.851776	-0.014742	1.784968
77.032739	936.047215	4.856781	-0.014800	1.791496
77.744867	944.185097	4.861786	-0.014938	1.798004
78.231724	952.301680	4.866790	-0.015034	1.804445
78.628280	960.443134	4.871795	-0.015113	1.810871
79.182842	968.594765	4.876800	-0.015222	1.817301
79.249126	976.770794	4.881805	-0.015239	1.823668
79.875184	984.877311	4.886810	-0.015361	1.830027
80.541067	993.001463	4.891814	-0.015490	1.836381
80.826219	1001.147391	4.896819	-0.015549	1.842685
81.321707	1009.288680	4.901824	-0.015646	1.848989
81.629514	1017.453409	4.906829	-0.015709	1.855267
82.428735	1025.520958	4.911834	-0.015863	1.861507
82.879533	1033.674232	4.916838	-0.015952	1.867750
83.531065	1041.809768	4.921843	-0.016079	1.873982
84.066734	1049.934464	4.926848	-0.016184	1.880172
84.468215	1058.061295	4.931853	-0.016264	1.886328
85.116809	1066.192370	4.936858	-0.016390	1.892495
85.485435	1074.327073	4.941862	-0.016463	1.898613
85.897541	1082.443987	4.946867	-0.016545	1.904703
86.544533	1090.568614	4.951872	-0.016671	1.910805
87.039027	1098.691054	4.956877	-0.016768	1.916868
87.437648	1106.809393	4.961882	-0.016848	1.922899
87.797400	1114.959022	4.966886	-0.016920	1.928930
88.140945	1123.088927	4.971891	-0.016989	1.934926
88.872180	1131.170098	4.976896	-0.017131	1.940909
89.397871	1139.286223	4.981901	-0.017234	1.946877
89.696634	1147.474855	4.986906	-0.017295	1.952855
90.184764	1155.594440	4.991910	-0.017391	1.958785
90.562764	1163.684029	4.996915	-0.017467	1.964664
91.100942	1171.787983	5.001920	-0.017572	1.970552
91.352675	1179.925332	5.006925	-0.017624	1.976416
91.755783	1188.032427	5.011930	-0.017704	1.982257
92.340548	1196.117731	5.016934	-0.017819	1.988084
92.599769	1204.256664	5.021939	-0.017872	1.993898
93.183202	1212.335161	5.026944	-0.017986	1.999686
93.646459	1220.409132	5.031949	-0.018077	2.005442
94.002635	1228.536277	5.036954	-0.018149	2.011207
94.210781	1236.694224	5.041958	-0.018193	2.016962
94.847375	1244.739572	5.046963	-0.018317	2.022666
95.400677	1252.854431	5.051968	-0.018425	2.028393
95.727310	1261.012782	5.056973	-0.018491	2.034112
96.419970	1269.059436	5.061978	-0.018625	2.039774
97.141995	1277.120436	5.066982	-0.018765	2.045433
97.626524	1285.221032	5.071987	-0.018860	2.051080
98.195368	1293.330446	5.076992	-0.018972	2.056725
98.355923	1301.460810	5.081997	-0.019007	2.062329
98.762909	1309.565644	5.087002	-0.019088	2.067924
99.211756	1317.686905	5.092006	-0.019177	2.073519
99.638826	1325.768748	5.097011	-0.019261	2.079070
100.133604	1333.837882	5.102016	-0.019359	2.084605
100.405422	1341.959121	5.107021	-0.019414	2.090138
101.152293	1350.024768	5.112026	-0.019559	2.095665
101.408482	1358.142707	5.117030	-0.019612	2.101165
101.766511	1366.234430	5.122035	-0.019684	2.106643
102.241845	1374.381614	5.127040	-0.019777	2.112154
102.660643	1382.491336	5.132045	-0.019861	2.117621
103.010802	1390.559862	5.137050	-0.019931	2.123040
103.143450	1398.674888	5.142054	-0.019961	2.128455
103.835241	1406.717329	5.147059	-0.020095	2.133861
104.006064	1414.842575	5.152064	-0.020132	2.139259
104.262826	1422.927938	5.157069	-0.020185	2.144625
104.871828	1430.972782	5.162074	-0.020304	2.149984
105.591033	1439.044092	5.167078	-0.020443	2.155357
105.699547	1447.138222	5.172083	-0.020468	2.160675
105.922938	1455.249908	5.177088	-0.020515	2.166001
106.155703	1463.359575	5.182093	-0.020564	2.171314
106.428980	1471.453054	5.187098	-0.020620	2.176607
106.611268	1479.558638	5.192102	-0.020659	2.181887
106.998249	1487.613797	5.197107	-0.020736	2.187140
107.269018	1495.750506	5.202112	-0.020792	2.192423
107.612639	1503.811922	5.207117	-0.020861	2.197651
108.007026	1511.858188	5.212122	-0.020940	2.202861
108.755573	1519.882767	5.217126	-0.021084	2.208076
108.854001	1527.993765	5.222131	-0.021108	2.213277
109.458384	1536.065207	5.227136	-0.021226	2.218485
109.801426	1544.146056	5.232141	-0.021295	2.223663
110.065151	1552.242588	5.237146	-0.021349	2.228832
110.219253	1560.380576	5.242150	-0.021383	2.234006
110.515738	1568.423082	5.247155	-0.021443	2.239119
111.046970	1576.473794	5.252160	-0.021547	2.244247
111.354771	1584.550310	5.257165	-0.021610	2.249360
111.506375	1592.668615	5.262170	-0.021643	2.254474
112.001322	1600.719474	5.267174	-0.021741	2.259563
112.314129	1608.780336	5.272179	-0.021804	2.264632
112.564500	1616.902684	5.277184	-0.021856	2.269722
112.772481	1625.064369	5.282189	-0.021900	2.274822
113.043183	1633.089224	5.287194	-0.021956	2.279830
113.128774	1641.162453	5.292198	-0.021977	2.284842
113.767519	1649.162277	5.297203	-0.022101	2.289844
114.223084	1657.244700	5.302208	-0.022191	2.294870
114.430340	1665.301303	5.307213	-0.022235	2.299849
114.995445	1673.329843	5.312218	-0.022345	2.304830
115.814112	1681.369534	5.317222	-0.022503	2.309828
116.180478	1689.466982	5.322227	-0.022576	2.314812
116.566647	1697.531582	5.327232	-0.022653	2.319767
117.060338	1705.578035	5.332237	-0.022751	2.324710
117.397186	1713.667903	5.337242	-0.022818	2.329655
117.814912	1721.760108	5.342246	-0.022902	2.334598
118.155778	1729.817181	5.347251	-0.022970	2.339502
118.502324	1737.905383	5.352256	-0.023040	2.344416
118.937825	1745.975710	5.357261	-0.023126	2.349316
119.091207	1754.102549	5.362266	-0.023160	2.354216
119.501995	1762.148501	5.367270	-0.023242	2.359079
119.638205	1770.215402	5.372275	-0.023272	2.363922
119.903724	1778.287333	5.377280	-0.023327	2.368768
120.337546	1786.350532	5.382285	-0.023413	2.373612
120.744637	1794.408887	5.387290	-0.023494	2.378442
121.269767	1802.462599	5.392294	-0.023597	2.383268
121.409777	1810.544092	5.397299	-0.023628	2.388071
121.954747	1818.625470	5.402304	-0.023735	2.392895
122.287374	1826.674794	5.407309	-0.023802	2.397674
122.701819	1834.716541	5.412314	-0.023884	2.402446
123.064307	1842.793677	5.417318	-0.023957	2.407225
123.123023	1850.897554	5.422323	-0.023973	2.411986
123.383633	1858.995046	5.427328	-0.024027	2.416750
123.747577	1867.022883	5.432333	-0.024100	2.421471
124.065519	1875.042446	5.437338	-0.024164	2.426175
124.430859	1883.139428	5.442342	-0.024238	2.430918
124.651362	1891.277172	5.447347	-0.024284	2.435665
125.290558	1899.249089	5.452352	-0.024408	2.440338
125.654089	1907.278797	5.457357	-0.024481	2.445015
125.881852	1915.348392	5.462362	-0.024529	2.449695
126.203963	1923.434517	5.467366	-0.024594	2.454383
126.468031	1931.479568	5.472371	-0.024648	2.459034
126.771821	1939.534309	5.477376	-0.024710	2.463685
127.091816	1947.596372	5.482381	-0.024775	2.468332
127.401873	1955.664490	5.487386	-0.024838	2.472973
127.691804	1963.738004	5.492390	-0.024897	2.477607
127.615065	1971.803643	5.497395	-0.024888	2.482201
128.093170	1979.830799	5.502400	-0.024982	2.486805
128.272944	1987.906180	5.507405	-0.025021	2.491406
128.496232	1995.981633	5.512410	-0.025068	2.496002
128.621498	2004.080051	5.517414	-0.025096	2.500595
129.121649	2012.051223	5.522419	-0.025194	2.505135
129.059196	2020.204431	5.527424	-0.025188	2.509729
129.607799	2028.235935	5.532429	-0.025295	2.514290
130.032917	2036.244794	5.537434	-0.025380	2.518820
130.424581	2044.272066	5.542438	-0.025458	2.523351
130.393196	2052.351252	5.547443	-0.025457	2.527872
130.641887	2060.418158	5.552448	-0.025509	2.532398
131.037139	2068.464496	5.557453	-0.025587	2.536915
131.426786	2076.502854	5.562458	-0.025665	2.541419
131.580851	2084.580536	5.567462	-0.025699	2.545920
131.759650	2092.638797	5.572467	-0.025738	2.550404
132.351497	2100.676635	5.577472	-0.025853	2.554898
132.545559	2108.734278	5.582477	-0.025894	2.559367
132.684092	2116.792185	5.587482	-0.025925	2.563824
133.089364	2124.842275	5.592486	-0.026006	2.568288
133.461842	2132.887173	5.597491	-0.026081	2.572739
133.815624	2140.940334	5.602496	-0.026152	2.577186
134.106508	2148.996122	5.607501	-0.026211	2.581621
134.417524	2157.056012	5.612506	-0.026274	2.586053
134.720829	2165.155772	5.617510	-0.026336	2.590498
134.870582	2173.391057	5.622515	-0.026369	2.594999
135.097187	2181.376328	5.627520	-0.026416	2.599362
135.339318	2189.375241	5.632525	-0.026467	2.603725
135.403244	2197.397736	5.637530	-0.026484	2.608082
135.720600	2205.442690	5.642534	-0.026548	2.612461
135.937475	2213.460603	5.647539	-0.026594	2.616811
136.512899	2221.478990	5.652544	-0.026706	2.621178
136.904858	2229.504146	5.657549	-0.026784	2.625529
137.245142	2237.525406	5.662554	-0.026853	2.629867
137.591469	2245.620169	5.667558	-0.026922	2.634238
137.916268	2253.638005	5.672563	-0.026988	2.638558
138.169511	2261.692248	5.677568	-0.027040	2.642887
138.525274	2269.744396	5.682573	-0.027112	2.647214
139.014162	2277.778465	5.687578	-0.027208	2.651533
139.339107	2285.852070	5.692582	-0.027274	2.655855
139.546719	2293.878107	5.697587	-0.027318	2.660137
139.987685	2301.910044	5.702592	-0.027405	2.664430
139.972205	2310.037085	5.707597	-0.027407	2.668738
140.261296	2318.096102	5.712602	-0.027466	2.673022
140.654519	2326.134354	5.717606	-0.027545	2.677295
140.921373	2334.158297	5.722611	-0.027600	2.681545
141.166378	2342.200733	5.727616	-0.027650	2.685797
141.496617	2350.236307	5.732621	-0.027717	2.690044
141.636653	2358.321309	5.737626	-0.027748	2.694298
142.146173	2366.340312	5.742630	-0.027848	2.698534
142.311442	2374.371641	5.747635	-0.027884	2.702748
142.668640	2382.418381	5.752640	-0.027956	2.706975
142.856660	2390.506484	5.757645	-0.027996	2.711207
143.015624	2398.558025	5.762650	-0.028031	2.715411
143.066820	2406.606128	5.767654	-0.028046	2.719601
143.475521	2414.620025	5.772659	-0.028127	2.723788
143.851335	2422.654614	5.777664	-0.028202	2.727977
144.062250	2430.728531	5.782669	-0.028247	2.732171
144.434310	2438.750617	5.787674	-0.028321	2.736340
144.942740	2446.789055	5.792678	-0.028421	2.740520
145.021966	2454.826334	5.797683	-0.028441	2.744667
145.241858	2462.899363	5.802688	-0.028487	2.748835
145.483285	2471.028465	5.807693	-0.028537	2.753026
145.624794	2479.085583	5.812698	-0.028569	2.757168
145.748781	2487.122798	5.817702	-0.028597	2.761293
146.089962	2495.100939	5.822707	-0.028666	2.765394
146.481040	2503.112225	5.827712	-0.028744	2.769509
146.718819	2511.198217	5.832717	-0.028793	2.773646
147.111889	2519.201690	5.837722	-0.028872	2.777745
147.485354	2527.252671	5.842726	-0.028947	2.781860
147.607017	2535.298786	5.847731	-0.028974	2.785952
147.880250	2543.333745	5.852736	-0.029030	2.790041
148.262905	2551.401360	5.857741	-0.029107	2.794147
148.315325	2559.470267	5.862746	-0.029122	2.798229
148.511403	2567.490523	5.867750	-0.029164	2.802288
148.882953	2575.493707	5.872755	-0.029238	2.806343
149.199494	2583.535472	5.877760	-0.029302	2.810408
149.497725	2591.602973	5.882765	-0.029363	2.814479
149.955126	2599.583835	5.887770	-0.029453	2.818510
150.263801	2607.650079	5.892774	-0.029516	2.822569
150.527952	2615.690095	5.897779	-0.029570	2.826607
150.827300	2623.779036	5.902784	-0.029631	2.830665
151.134366	2631.859472	5.907789	-0.029694	2.834714
151.573442	2639.825067	5.912794	-0.029780	2.838707
151.683617	2647.878859	5.917798	-0.029806	2.842720
151.557273	2655.966377	5.922803	-0.029788	2.846730
152.085349	2663.960685	5.927808	-0.029891	2.850725
152.459644	2672.002714	5.932813	-0.029966	2.854730
152.880394	2680.020721	5.937818	-0.030050	2.858719
153.131281	2688.081846	5.942822	-0.030102	2.862715
153.217106	2696.142436	5.947827	-0.030123	2.866696
153.315645	2704.212232	5.952832	-0.030146	2.870677
153.751688	2712.239806	5.957837	-0.030233	2.874649
154.005025	2720.251990	5.962842	-0.030285	2.878599
154.382262	2728.280673	5.967846	-0.030361	2.882558
154.595103	2736.317146	5.972851	-0.030405	2.886507
154.868165	2744.378519	5.977856	-0.030461	2.890465
155.161750	2752.418776	5.982861	-0.030521	2.894409
155.491653	2760.456557	5.987866	-0.030588	2.898348
155.795694	2768.488427	5.992870	-0.030650	2.902277
156.018717	2776.531265	5.997875	-0.030696	2.906202
156.370591	2784.556829	6.002880	-0.030767	2.910120
156.777318	2792.689135	6.007885	-0.030848	2.914088
157.009614	2800.668703	6.012890	-0.030897	2.917966
157.280681	2808.727746	6.017894	-0.030952	2.921880
157.445475	2816.741438	6.022899	-0.030988	2.925762
157.724958	2824.761172	6.027904	-0.031045	2.929647
157.842722	2832.839717	6.032909	-0.031072	2.933546
158.078759	2840.850721	6.037914	-0.031122	2.937415
158.695792	2848.859837	6.042918	-0.031242	2.941296
158.866438	2856.878570	6.047923	-0.031279	2.945155
158.963418	2864.944521	6.052928	-0.031302	2.949027
159.408602	2873.002628	6.057933	-0.031390	2.952907
159.901606	2881.013528	6.062938	-0.031487	2.956763
159.997753	2889.085507	6.067942	-0.031510	2.960623
159.944792	2897.101478	6.072947	-0.031505	2.964443
160.286448	2905.134855	6.077952	-0.031574	2.968286
160.620049	2913.198081	6.082957	-0.031642	2.972138
160.859840	2921.218136	6.087962	-0.031691	2.975960
161.122211	2929.250191	6.092966	-0.031745	2.979784
161.442494	2937.274707	6.097971	-0.031810	2.983602
161.457068	2945.347940	6.102976	-0.031818	2.987423
161.819369	2953.377645	6.107981	-0.031891	2.991236
162.137059	2961.409255	6.112986	-0.031955	2.995043
162.433466	2969.451508	6.117990	-0.032016	2.998849
162.305545	2977.506861	6.122995	-0.031997	3.002635
162.597016	2985.525738	6.128000	-0.032056	3.006420
163.053749	2993.510331	6.133005	-0.032147	3.010192
163.275864	3001.572960	6.138010	-0.032193	3.013984
163.872931	3009.594148	6.143014	-0.032309	3.017770
163.941946	3017.655912	6.148019	-0.032328	3.021545
164.238302	3025.652733	6.153024	-0.032388	3.025296
164.589466	3033.705510	6.158029	-0.032458	3.029071
164.823435	3041.775945	6.163034	-0.032507	3.032843
165.013988	3049.844259	6.168038	-0.032548	3.036608
165.153363	3057.848672	6.173043	-0.032579	3.040336
165.497046	3065.841994	6.178048	-0.032648	3.044064
165.905625	3073.879060	6.183053	-0.032729	3.047811
165.943871	3081.944587	6.188058	-0.032742	3.051548
166.172054	3089.995222	6.193062	-0.032790	3.055284
166.430361	3097.987182	6.198067	-0.032843	3.058988
166.690540	3106.050379	6.203072	-0.032896	3.062722
167.002884	3114.078949	6.208077	-0.032960	3.066437
167.096295	3122.098228	6.213082	-0.032982	3.070133
167.469804	3130.237480	6.218086	-0.033057	3.073893
167.515212	3138.266302	6.223091	-0.033071	3.077582
167.700985	3146.266804	6.228096	-0.033111	3.081261
167.999610	3154.255387	6.233101	-0.033171	3.084934
167.999332	3162.287078	6.238106	-0.033176	3.088609
168.468425	3170.321633	6.243110	-0.033269	3.092303
168.748185	3178.352131	6.248115	-0.033326	3.095982
169.111089	3186.381292	6.253120	-0.033399	3.099659
169.383015	3194.397003	6.258125	-0.033455	3.103322
169.774417	3202.409079	6.263130	-0.033533	3.106984
170.063387	3210.480171	6.268134	-0.033592	3.110664
169.959463	3218.546875	6.273139	-0.033578	3.114320
170.434715	3226.554745	6.278144	-0.033671	3.117971
170.674645	3234.591321	6.283149	-0.033721	3.121620
170.695506	3242.616162	6.288154	-0.033730	3.125249
171.175005	3250.641950	6.293158	-0.033825	3.128895
171.473680	3258.679845	6.298163	-0.033886	3.132535
171.765624	3266.739691	6.303168	-0.033945	3.136179
172.078598	3274.726503	6.308173	-0.034009	3.139788
172.631713	3282.741652	6.313178	-0.034117	3.143415
172.821416	3290.809343	6.318182	-0.034157	3.147046
173.164015	3298.827737	6.323187	-0.034226	3.150657
173.211732	3306.923120	6.328192	-0.034240	3.154286
173.667952	3314.926938	6.333197	-0.034331	3.157887
173.779620	3322.935626	6.338202	-0.034357	3.161472
174.000425	3330.942259	6.343206	-0.034403	3.165056
174.222469	3338.999295	6.348211	-0.034449	3.168658
174.528037	3347.006418	6.353216	-0.034511	3.172238
174.649031	3355.101486	6.358221	-0.034539	3.175845
174.745738	3363.114661	6.363226	-0.034562	3.179410
175.510433	3371.106308	6.368230	-0.034710	3.182990
175.607285	3379.149008	6.373235	-0.034733	3.186560
175.949866	3387.157719	6.378240	-0.034802	3.190122
176.201523	3395.256893	6.383245	-0.034854	3.193716
176.300813	3403.269450	6.388250	-0.034878	3.197261
176.629420	3411.314621	6.393254	-0.034944	3.200826
176.709052	3419.307350	6.398259	-0.034964	3.204353
177.009998	3427.339921	6.403264	-0.035025	3.207904
177.246712	3435.404609	6.408269	-0.035075	3.211461
177.453238	3443.426455	6.413274	-0.035118	3.214995
177.995963	3451.460732	6.418278	-0.035225	3.218544
177.961383	3459.490949	6.423283	-0.035223	3.222064
178.236870	3467.503263	6.428288	-0.035280	3.225585
178.600971	3475.549813	6.433293	-0.035353	3.229120
178.675989	3483.622111	6.438298	-0.035372	3.232651
178.818118	3491.692790	6.443302	-0.035404	3.236180
179.134725	3499.618751	6.448307	-0.035468	3.239649
179.454475	3507.623353	6.453312	-0.035532	3.243149
179.450868	3515.696582	6.458317	-0.035537	3.246662
179.773016	3523.674719	6.463322	-0.035602	3.250143
180.205391	3531.747185	6.468326	-0.035688	3.253665
180.396038	3539.788717	6.473331	-0.035729	3.257160
180.734868	3547.783694	6.478336	-0.035797	3.260638
180.990307	3555.823816	6.483341	-0.035850	3.264127
181.317425	3563.838006	6.488346	-0.035916	3.267605
181.353632	3571.928417	6.493350	-0.035928	3.271100
181.626131	3579.922208	6.498355	-0.035984	3.274560
181.859940	3587.959965	6.503360	-0.036032	3.278033
181.873911	3596.029732	6.508365	-0.036040	3.281507
182.243117	3603.968740	6.513370	-0.036114	3.284935
182.664438	3612.003189	6.518374	-0.036198	3.288403
182.886347	3620.061204	6.523379	-0.036244	3.291869
183.043399	3628.108825	6.528384	-0.036279	3.295325
183.491159	3636.145729	6.533389	-0.036367	3.298784
183.464155	3644.152301	6.538394	-0.036367	3.302207
183.825716	3652.179609	6.543398	-0.036440	3.305651
184.020454	3660.219941	6.548403	-0.036481	3.309091
184.673418	3668.232808	6.553408	-0.036608	3.312532
184.974646	3676.319683	6.558413	-0.036669	3.315988
185.100136	3684.286669	6.563418	-0.036698	3.319383
185.595950	3692.288292	6.568422	-0.036795	3.322803
185.789819	3700.337244	6.573427	-0.036837	3.326228
186.080312	3708.339796	6.578432	-0.036896	3.329634
186.339733	3716.410142	6.583437	-0.036949	3.333063
186.537046	3724.459634	6.588442	-0.036991	3.336478
186.740268	3732.471169	6.593446	-0.037034	3.339874
186.914917	3740.491208	6.598451	-0.037072	3.343268
187.230406	3748.522914	6.603456	-0.037136	3.346669
187.439969	3756.549074	6.608461	-0.037180	3.350061
187.381211	3764.634637	6.613466	-0.037174	3.353464
187.885722	3772.666158	6.618470	-0.037274	3.356861
188.150081	3780.658168	6.623475	-0.037328	3.360230
188.554356	3788.637504	6.628480	-0.037408	3.363595
188.697021	3796.709035	6.633485	-0.037440	3.366986
188.841248	3804.726778	6.638490	-0.037472	3.370350
189.271024	3812.797137	6.643494	-0.037557	3.373744
189.283286	3820.834832	6.648499	-0.037565	3.377106
189.436373	3828.855253	6.653504	-0.037599	3.380462
189.705652	3836.856016	6.658509	-0.037654	3.383811
189.828205	3844.883860	6.663514	-0.037682	3.387162
190.240737	3852.925508	6.668518	-0.037764	3.390526
190.618170	3861.010549	6.673523	-0.037839	3.393904
190.625162	3869.015887	6.678528	-0.037846	3.397232
190.957192	3877.022451	6.683533	-0.037913	3.400568
191.343730	3884.979834	6.688538	-0.037990	3.403883
191.644451	3893.001981	6.693542	-0.038051	3.407218
191.697349	3901.042727	6.698547	-0.038066	3.410549
192.119785	3909.061781	6.703552	-0.038150	3.413881
192.480835	3917.112043	6.708557	-0.038223	3.417220
192.606921	3925.103305	6.713562	-0.038251	3.420523
193.189082	3933.120468	6.718566	-0.038365	3.423849
193.471073	3941.157230	6.723571	-0.038422	3.427170
193.540221	3949.210846	6.728576	-0.038441	3.430487
193.884431	3957.278142	6.733581	-0.038510	3.433816
194.091482	3965.280878	6.738586	-0.038554	3.437111
194.368562	3973.287278	6.743590	-0.038610	3.440406
194.379404	3981.319071	6.748595	-0.038618	3.443700
194.502323	3989.373221	6.753600	-0.038646	3.447003
194.731460	3997.394615	6.758605	-0.038693	3.450294
194.878401	4005.445615	6.763610	-0.038726	3.453590
195.157749	4013.466322	6.768614	-0.038783	3.456876
195.496691	4021.481649	6.773619	-0.038852	3.460157
195.849157	4029.473035	6.778624	-0.038922	3.463427
196.136182	4037.530992	6.783629	-0.038981	3.466718
196.360765	4045.554842	6.788634	-0.039028	3.469990
196.654691	4053.650849	6.793638	-0.039088	3.473291
196.819352	4061.680234	6.798643	-0.039124	3.476557
197.098329	4069.589768	6.803648	-0.039181	3.479775
197.400710	4077.650563	6.808653	-0.039242	3.483052
197.326144	4085.652780	6.813658	-0.039234	3.486291
197.526747	4093.686609	6.818662	-0.039276	3.489548
197.782657	4101.730718	6.823667	-0.039329	3.492807
197.991973	4109.748940	6.828672	-0.039373	3.496052
198.063851	4117.793812	6.833677	-0.039392	3.499300
198.404101	4125.779874	6.838682	-0.039460	3.502530
198.727467	4133.829055	6.843686	-0.039526	3.505781
198.737688	4141.862436	6.848691	-0.039533	3.509014
198.982500	4149.862826	6.853696	-0.039584	3.512237
199.271635	4157.924093	6.858701	-0.039643	3.515484
199.317518	4165.925761	6.863706	-0.039656	3.518696
199.701754	4173.927106	6.868710	-0.039733	3.521915
200.092422	4181.924552	6.873715	-0.039811	3.525129
200.249418	4189.957991	6.878720	-0.039845	3.528349
200.693215	4198.019522	6.883725	-0.039933	3.531584
200.950694	4206.038472	6.888730	-0.039986	3.534795
201.175771	4214.111875	6.893734	-0.040033	3.538023
201.443868	4222.132365	6.898739	-0.040088	3.541228
201.501695	4230.112341	6.903744	-0.040104	3.544408
201.977072	4238.185555	6.908749	-0.040198	3.547635
201.930692	4246.207453	6.913754	-0.040195	3.550823
202.021812	4254.379757	6.918758	-0.040217	3.554072
202.362311	4262.335849	6.923763	-0.040285	3.557239
202.418562	4270.286930	6.928768	-0.040301	3.560393
202.679742	4278.311334	6.933773	-0.040355	3.563579
203.015946	4286.300489	6.938778	-0.040423	3.566751
203.195484	4294.312249	6.943782	-0.040461	3.569924
203.383695	4302.379614	6.948787	-0.040502	3.573117
203.641464	4310.401784	6.953792	-0.040555	3.576291
204.169877	4318.378434	6.958797	-0.040658	3.579451
204.312779	4326.389298	6.963802	-0.040690	3.582612
204.860321	4334.417183	6.968806	-0.040797	3.585787
205.087222	4342.441214	6.973811	-0.040845	3.588950
205.249992	4350.505618	6.978816	-0.040880	3.592123
205.475838	4358.561613	6.983821	-0.040927	3.595292
205.532205	4366.546865	6.988826	-0.040943	3.598426
205.971231	4374.582987	6.993830	-0.041030	3.601588
206.117895	4382.540901	6.998835	-0.041062	3.604708
206.501057	4390.568192	7.003840	-0.041139	3.607859
206.862023	4398.638599	7.008845	-0.041211	3.611024
206.690910	4406.668678	7.013850	-0.041185	3.614155
207.053673	4414.719662	7.018854	-0.041257	3.617306
207.428093	4422.707329	7.023859	-0.041332	3.620430
207.937037	4430.684728	7.028864	-0.041432	3.623551
208.160860	4438.772416	7.033869	-0.041479	3.626705
208.344698	4446.756748	7.038874	-0.041519	3.629815
208.819333	4454.851037	7.043878	-0.041612	3.632972
208.944437	4462.921021	7.048883	-0.041641	3.636108
209.144455	4470.837483	7.053888	-0.041683	3.639183
209.544439	4478.897843	7.058893	-0.041763	3.642317
209.767630	4486.862787	7.063898	-0.041809	3.645406
210.019281	4494.903720	7.068902	-0.041861	3.648523
210.410721	4502.964837	7.073907	-0.041940	3.651649
210.448047	4511.005128	7.078912	-0.041952	3.654755
210.539520	4519.038931	7.083917	-0.041974	3.657857
210.653631	4527.031096	7.088922	-0.042000	3.660941
211.169736	4535.051063	7.093926	-0.042102	3.664043
211.334422	4543.084415	7.098931	-0.042137	3.667139
211.227791	4551.119898	7.103936	-0.042123	3.670226
211.566747	4559.172457	7.108941	-0.042191	3.673328
211.880929	4567.196189	7.113946	-0.042255	3.676416
211.820752	4575.185478	7.118950	-0.042249	3.679479
212.276584	4583.191574	7.123955	-0.042339	3.682559
212.261408	4591.209276	7.128960	-0.042341	3.685628
212.532797	4599.250904	7.133965	-0.042397	3.688711
212.740482	4607.263491	7.138970	-0.042441	3.691779
213.033717	4615.310012	7.143974	-0.042501	3.694860
213.189620	4623.337882	7.148979	-0.042535	3.697927
213.329474	4631.344039	7.153984	-0.042566	3.700983
213.731093	4639.344995	7.158989	-0.042646	3.704041
213.706830	4647.384112	7.163994	-0.042647	3.707101
213.896003	4655.408856	7.168998	-0.042687	3.710158
213.992591	4663.497154	7.174003	-0.042710	3.713234
214.234521	4671.538576	7.179008	-0.042760	3.716293
214.577254	4679.496397	7.184013	-0.042829	3.719320
214.547918	4687.513970	7.189018	-0.042829	3.722359
214.900656	4695.483574	7.194022	-0.042900	3.725386
215.305558	4703.486265	7.199027	-0.042981	3.728425
215.404723	4711.556882	7.204032	-0.043004	3.731479
215.757391	4719.587801	7.209037	-0.043075	3.734522
215.801763	4727.605678	7.214042	-0.043088	3.737550
215.827160	4735.651956	7.219046	-0.043098	3.740585
216.113394	4743.658878	7.224051	-0.043157	3.743610
216.573231	4751.665887	7.229056	-0.043248	3.746636
216.754915	4759.723179	7.234061	-0.043287	3.749672
216.907123	4767.729080	7.239066	-0.043320	3.752686
217.176642	4775.765943	7.244070	-0.043376	3.755711
217.384906	4783.766536	7.249075	-0.043420	3.758720
217.317224	4791.826961	7.254080	-0.043412	3.761741
217.750883	4799.786959	7.259085	-0.043498	3.764734
217.937411	4807.852572	7.264090	-0.043538	3.767759
218.277569	4815.887177	7.269094	-0.043607	3.770773
218.534269	4823.904111	7.274099	-0.043659	3.773776
218.740582	4831.945597	7.279104	-0.043703	3.776785
219.063760	4839.936462	7.284109	-0.043768	3.779775
219.202915	4847.973985	7.289114	-0.043800	3.782776
219.407676	4855.987278	7.294118	-0.043843	3.785766
219.776924	4864.019157	7.299123	-0.043917	3.788765
219.838049	4872.067200	7.304128	-0.043933	3.791761
220.181963	4880.106835	7.309133	-0.044003	3.794758
220.301774	4888.094544	7.314138	-0.044030	3.797728
220.414258	4896.079733	7.319142	-0.044056	3.800694
220.606658	4904.099445	7.324147	-0.044097	3.803673
220.726973	4912.115355	7.329152	-0.044125	3.806646
220.871567	4920.170778	7.334157	-0.044157	3.809633
220.822430	4928.179513	7.339162	-0.044153	3.812595
220.987419	4936.223662	7.344166	-0.044189	3.815573
221.399505	4944.164630	7.349171	-0.044271	3.818515
221.755184	4952.181088	7.354176	-0.044342	3.821482
222.000325	4960.184766	7.359181	-0.044393	3.824440
222.090996	4968.256808	7.364186	-0.044415	3.827417
222.542641	4976.242906	7.369190	-0.044504	3.830367
222.745467	4984.307796	7.374195	-0.044547	3.833339
222.864327	4992.327650	7.379200	-0.044575	3.836291
223.126876	5000.357685	7.384205	-0.044629	3.839247
223.064690	5008.374514	7.389210	-0.044622	3.842189
223.294628	5016.327780	7.394214	-0.044670	3.845112
223.626979	5024.400015	7.399219	-0.044737	3.848078
223.836449	5032.415422	7.404224	-0.044781	3.851018
224.041653	5040.489334	7.409229	-0.044825	3.853977
224.375849	5048.498516	7.414234	-0.044892	3.856913
224.822403	5056.471995	7.419238	-0.044981	3.859836
224.986640	5064.513940	7.424243	-0.045016	3.862776
225.045177	5072.515545	7.429248	-0.045032	3.865697
225.305536	5080.624668	7.434253	-0.045086	3.868659
225.493017	5088.635136	7.439258	-0.045126	3.871581
225.932040	5096.888915	7.444262	-0.045213	3.874594
226.025002	5104.845635	7.449267	-0.045236	3.877491
226.185301	5112.732639	7.454272	-0.045271	3.880361
226.338889	5120.733385	7.459277	-0.045304	3.883270
226.752985	5128.691325	7.464282	-0.045387	3.886166
227.044122	5136.704837	7.469286	-0.045446	3.889078
227.193258	5144.772350	7.474291	-0.045479	3.892004
227.362425	5152.782878	7.479296	-0.045516	3.894908
227.712992	5160.822934	7.484301	-0.045586	3.897824
227.771364	5168.811584	7.489306	-0.045602	3.900714
228.157068	5176.790351	7.494310	-0.045679	3.903604
228.363587	5184.832753	7.499315	-0.045723	3.906512
228.424899	5192.857432	7.504320	-0.045739	3.909408
228.377884	5200.918682	7.509325	-0.045736	3.912313
228.638871	5208.938359	7.514330	-0.045790	3.915207
228.999339	5216.948699	7.519334	-0.045862	3.918097
229.174079	5224.983925	7.524339	-0.045900	3.920991
229.247285	5232.933763	7.529344	-0.045918	3.923849
229.549454	5240.976370	7.534349	-0.045980	3.926744
229.663216	5248.933388	7.539354	-0.046006	3.929601
229.812615	5257.038189	7.544358	-0.046039	3.932511
230.052163	5265.082786	7.549363	-0.046089	3.935398
230.195120	5273.051763	7.554368	-0.046121	3.938254
230.490106	5281.073333	7.559373	-0.046181	3.941130
230.585747	5289.072965	7.564378	-0.046204	3.943992
230.919935	5297.129041	7.569382	-0.046271	3.946877
231.167611	5305.156819	7.574387	-0.046323	3.949747
231.277190	5313.193635	7.579392	-0.046348	3.952617
231.570492	5321.254774	7.584397	-0.046408	3.955496
231.561413	5329.210868	7.589402	-0.046412	3.958330
231.766595	5337.186261	7.594406	-0.046455	3.961173
232.289371	5345.201742	7.599411	-0.046557	3.964034
232.494244	5353.220521	7.604416	-0.046601	3.966888
232.777516	5361.220423	7.609421	-0.046659	3.969734
233.011632	5369.275101	7.614426	-0.046707	3.972598
233.330323	5377.290417	7.619430	-0.046772	3.975446
233.582215	5385.341124	7.624435	-0.046824	3.978304
233.790195	5393.325681	7.629440	-0.046868	3.981136
234.242289	5401.363138	7.634445	-0.046957	3.983988
234.160189	5409.418407	7.639450	-0.046947	3.986836
234.323387	5417.442714	7.644454	-0.046983	3.989675
234.633448	5425.475939	7.649459	-0.047046	3.992517
234.799527	5433.493154	7.654464	-0.047082	3.995349
235.021788	5441.551710	7.659469	-0.047128	3.998195
235.269261	5449.547645	7.664474	-0.047180	4.001017
235.615726	5457.494421	7.669478	-0.047249	4.003821
235.539066	5465.604839	7.674483	-0.047240	4.006674
235.818514	5473.581997	7.679488	-0.047298	4.009484
236.316239	5481.614019	7.684493	-0.047395	4.012315
236.286825	5489.646331	7.689498	-0.047395	4.015135
236.569372	5497.666370	7.694502	-0.047453	4.017954
236.833287	5505.687626	7.699507	-0.047507	4.020771
237.180774	5513.634410	7.704512	-0.047577	4.023561
237.190876	5521.702001	7.709517	-0.047584	4.026386
237.253036	5529.746292	7.714522	-0.047601	4.029202
237.658794	5537.773714	7.719526	-0.047682	4.032016
237.826063	5545.884854	7.724531	-0.047718	4.034853
237.935372	5553.856640	7.729536	-0.047744	4.037638
238.233916	5561.782261	7.734541	-0.047804	4.040408
238.342581	5569.788480	7.739546	-0.047830	4.043202
238.376486	5577.814124	7.744550	-0.047841	4.045999
238.787120	5585.863079	7.749555	-0.047923	4.048808
238.864903	5593.852412	7.754560	-0.047942	4.051589
239.064054	5601.904311	7.759565	-0.047985	4.054392
239.212498	5609.922584	7.764570	-0.048018	4.057181
239.467508	5617.868415	7.769574	-0.048070	4.059944
239.643542	5625.915624	7.774579	-0.048108	4.062739
239.820901	5633.928780	7.779584	-0.048146	4.065520
240.103716	5641.969460	7.784589	-0.048204	4.068311
240.401716	5649.998055	7.789594	-0.048265	4.071095
240.342616	5658.039069	7.794598	-0.048259	4.073877
240.435132	5666.070614	7.799603	-0.048281	4.076656
240.612969	5673.999547	7.804608	-0.048320	4.079399
240.916879	5682.083655	7.809613	-0.048382	4.082195
240.770800	5690.049579	7.814618	-0.048359	4.084942
241.217903	5698.105876	7.819622	-0.048448	4.087727
241.533948	5706.121199	7.824627	-0.048512	4.090494
241.372001	5714.137517	7.829632	-0.048487	4.093252
241.595725	5722.204542	7.834637	-0.048534	4.096032
241.670077	5730.163801	7.839642	-0.048553	4.098771
241.814737	5738.237555	7.844646	-0.048585	4.101548
241.908715	5746.203260	7.849651	-0.048608	4.104285
242.006279	5754.222417	7.854656	-0.048631	4.107039
242.465699	5762.240104	7.859661	-0.048722	4.109795
242.618186	5770.308279	7.864666	-0.048755	4.112563
242.751562	5778.342541	7.869670	-0.048785	4.115317
243.108272	5786.371451	7.874675	-0.048857	4.118070
243.112511	5794.347335	7.879680	-0.048863	4.120798
243.388882	5802.365389	7.884685	-0.048919	4.123543
243.551973	5810.375560	7.889690	-0.048955	4.126281
243.676528	5818.392489	7.894694	-0.048983	4.129020
243.691078	5826.461683	7.899699	-0.048991	4.131773
243.950747	5834.446195	7.904704	-0.049045	4.134499
244.175453	5842.517045	7.909709	-0.049092	4.137251
244.196321	5850.494933	7.914714	-0.049101	4.139968
244.554690	5858.536245	7.919718	-0.049173	4.142709
244.783280	5866.530525	7.924723	-0.049221	4.145430
244.852146	5874.522715	7.929728	-0.049239	4.148147
244.992535	5882.596853	7.934733	-0.049270	4.150890
245.126247	5890.625090	7.939738	-0.049300	4.153616
245.321701	5898.617932	7.944742	-0.049342	4.156329
245.603926	5906.639929	7.949747	-0.049399	4.159051
245.740151	5914.646300	7.954752	-0.049430	4.161765
246.181329	5922.621215	7.959757	-0.049517	4.164469
246.271930	5930.653539	7.964762	-0.049539	4.167187
246.397267	5938.649379	7.969766	-0.049568	4.169891
246.848192	5946.713955	7.974771	-0.049657	4.172621
246.639472	5954.747735	7.979776	-0.049623	4.175331
246.867748	5962.771848	7.984781	-0.049671	4.178040
246.969589	5970.751538	7.989786	-0.049695	4.180732
247.248857	5978.765148	7.994790	-0.049752	4.183435
247.322412	5986.809954	7.999795	-0.049771	4.186144
247.605474	5994.795050	8.004800	-0.049829	4.188834
247.898573	6002.816669	8.009805	-0.049889	4.191535
247.881533	6010.966452	8.014810	-0.049891	4.194273
248.130721	6018.981424	8.019814	-0.049942	4.196968
248.514307	6026.906407	8.024819	-0.050019	4.199631
248.430170	6034.907415	8.029824	-0.050008	4.202314
248.541911	6042.895559	8.034829	-0.050034	4.204993
248.767101	6050.903205	8.039834	-0.050081	4.207677
248.931646	6058.916915	8.044838	-0.050117	4.210362
249.049556	6066.991320	8.049843	-0.050144	4.213064
249.259157	6074.999181	8.054848	-0.050189	4.215743
249.676228	6083.020271	8.059853	-0.050272	4.218427
249.709215	6090.979077	8.064858	-0.050283	4.221085
249.976046	6098.990554	8.069862	-0.050338	4.223761
250.169733	6107.061737	8.074867	-0.050379	4.226454
250.321228	6115.016579	8.079872	-0.050412	4.229107
250.234954	6123.141574	8.084877	-0.050401	4.231812
250.558265	6131.146885	8.089882	-0.050467	4.234479
250.839796	6139.150079	8.094886	-0.050524	4.237144
250.976243	6147.145477	8.099891	-0.050555	4.239803
251.288816	6155.134612	8.104896	-0.050618	4.242460
251.586614	6163.153745	8.109901	-0.050679	4.245125
251.671652	6171.195955	8.114906	-0.050700	4.247794
251.776722	6179.166444	8.119910	-0.050725	4.250437
252.133703	6187.274813	8.124915	-0.050796	4.253127
252.105738	6195.282509	8.129920	-0.050796	4.255779
252.319362	6203.286112	8.134925	-0.050841	4.258430
252.514098	6211.282062	8.139930	-0.050883	4.261076
252.533169	6219.316835	8.144934	-0.050892	4.263732
252.892283	6227.369781	8.149939	-0.050964	4.266395
252.895116	6235.358331	8.154944	-0.050969	4.269032
253.222794	6243.403380	8.159949	-0.051035	4.271689
253.332274	6251.476018	8.164954	-0.051061	4.274351
253.345484	6259.493544	8.169958	-0.051069	4.276993
253.660603	6267.436626	8.174963	-0.051133	4.279611
253.646003	6275.465726	8.179968	-0.051135	4.282253
254.024085	6283.428675	8.184973	-0.051211	4.284875
254.234668	6291.492801	8.189978	-0.051255	4.287527
254.387257	6299.464498	8.194982	-0.051289	4.290147
254.493103	6307.572561	8.199987	-0.051313	4.292809
254.661976	6315.502432	8.204992	-0.051350	4.295412
255.205718	6323.582902	8.209997	-0.051457	4.298066
255.277726	6331.590677	8.215002	-0.051475	4.300690
255.340593	6339.582605	8.220006	-0.051492	4.303307
255.724981	6347.622827	8.225011	-0.051569	4.305941
255.849100	6355.614696	8.230016	-0.051597	4.308556
255.993468	6363.667405	8.235021	-0.051629	4.311189
256.031226	6371.714994	8.240026	-0.051641	4.313818
256.286468	6379.684384	8.245030	-0.051694	4.316422
256.344020	6387.720351	8.250035	-0.051710	4.319044
256.376212	6395.696638	8.255040	-0.051721	4.321645
256.676153	6403.709515	8.260045	-0.051782	4.324258
256.839575	6411.752259	8.265050	-0.051818	4.326878
256.951222	6419.722335	8.270054	-0.051844	4.329473
257.207728	6427.817189	8.275059	-0.051897	4.332108
257.292999	6435.800448	8.280064	-0.051918	4.334703
257.389476	6443.830608	8.285069	-0.051941	4.337313
257.590295	6451.825110	8.290074	-0.051983	4.339909
257.706644	6459.851168	8.295078	-0.052010	4.342514
257.961956	6467.845698	8.300083	-0.052063	4.345108
258.093863	6475.858085	8.305088	-0.052093	4.347706
258.555833	6483.910516	8.310093	-0.052184	4.350317
258.581524	6491.962673	8.315098	-0.052194	4.352923
258.730493	6500.010625	8.320102	-0.052227	4.355528
258.930849	6508.032570	8.325107	-0.052269	4.358123
259.026359	6515.912449	8.330112	-0.052292	4.360669
259.208419	6523.952089	8.335117	-0.052331	4.363266
259.006102	6531.997645	8.340122	-0.052299	4.365862
259.505388	6540.002628	8.345126	-0.052397	4.368446
259.537454	6548.044924	8.350131	-0.052408	4.371039
259.478538	6555.995673	8.355136	-0.052402	4.373600
259.764867	6564.065462	8.360141	-0.052461	4.376200
260.083329	6572.086251	8.365146	-0.052525	4.378782
260.296712	6580.068986	8.370150	-0.052570	4.381350
260.330639	6588.080828	8.375155	-0.052582	4.383925
260.779842	6596.098432	8.380160	-0.052670	4.386503
260.891416	6604.134143	8.385165	-0.052696	4.389083
260.776407	6612.205483	8.390170	-0.052680	4.391672
261.114600	6620.187763	8.395174	-0.052748	4.394233
261.285534	6628.247600	8.400179	-0.052785	4.396816
261.348783	6636.220281	8.405184	-0.052802	4.399370
261.648538	6644.256510	8.410189	-0.052863	4.401943
261.976286	6652.214167	8.415194	-0.052929	4.404490
261.904785	6660.257648	8.420198	-0.052921	4.407061
262.100502	6668.272612	8.425203	-0.052963	4.409622
262.168894	6676.325438	8.430208	-0.052981	4.412194
262.496136	6684.322592	8.435213	-0.053047	4.414748
262.525125	6692.375659	8.440218	-0.053058	4.417316
262.675723	6700.324972	8.445222	-0.053091	4.419850
263.036393	6708.412346	8.450227	-0.053163	4.422428
262.970015	6716.376868	8.455232	-0.053156	4.424964
263.257010	6724.443382	8.460237	-0.053215	4.427532
263.594622	6732.419771	8.465242	-0.053283	4.430069
263.708503	6740.477417	8.470246	-0.053309	4.432631
264.024902	6748.541175	8.475251	-0.053373	4.435193
263.983780	6756.535434	8.480256	-0.053371	4.437731
264.193747	6764.498733	8.485261	-0.053415	4.440258
264.175243	6772.535372	8.490266	-0.053417	4.442806
264.254749	6780.511421	8.495270	-0.053437	4.445334
264.484004	6788.570191	8.500275	-0.053485	4.447887
264.363655	6796.542940	8.505280	-0.053467	4.450411
264.478323	6804.637989	8.510285	-0.053494	4.452972
264.970294	6812.622010	8.515290	-0.053591	4.455498
264.936159	6820.641126	8.520294	-0.053589	4.458032
265.210555	6828.669455	8.525299	-0.053646	4.460568
265.270342	6836.658189	8.530304	-0.053662	4.463090
265.421056	6844.679258	8.535309	-0.053695	4.465620
265.603628	6852.699675	8.540314	-0.053734	4.468149
265.796443	6860.668123	8.545318	-0.053775	4.470661
265.967681	6868.768278	8.550323	-0.053813	4.473212
266.005778	6876.756303	8.555328	-0.053825	4.475726
266.202807	6884.763268	8.560333	-0.053867	4.478245
266.383411	6892.799810	8.565338	-0.053906	4.480772
266.531286	6900.778637	8.570343	-0.053938	4.483280
266.526065	6908.770274	8.575347	-0.053942	4.485789
266.691348	6916.812723	8.580352	-0.053978	4.488314
267.201655	6924.820108	8.585357	-0.054079	4.490826
267.294018	6932.880360	8.590362	-0.054101	4.493353
267.255726	6940.859494	8.595367	-0.054099	4.495853
267.775801	6948.905637	8.600371	-0.054201	4.498374
267.801803	6956.861375	8.605376	-0.054211	4.500864
267.986120	6964.877307	8.610381	-0.054250	4.503371
268.085860	6972.918360	8.615386	-0.054274	4.505885
268.293859	6980.972210	8.620391	-0.054318	4.508402
268.456342	6989.013949	8.625395	-0.054354	4.510913
268.753618	6997.017347	8.630400	-0.054414	4.513411
269.010063	7005.054595	8.635405	-0.054467	4.515919
269.035636	7013.005644	8.640410	-0.054477	4.518397
269.111008	7020.987850	8.645415	-0.054496	4.520884
269.398419	7029.010402	8.650419	-0.054555	4.523383
269.161468	7037.011263	8.655424	-0.054516	4.525872
269.347302	7045.050371	8.660429	-0.054556	4.528373
269.758573	7053.059713	8.665434	-0.054637	4.530863
269.897465	7061.090032	8.670439	-0.054669	4.533358
270.008301	7069.126980	8.675443	-0.054694	4.535854
270.132187	7077.118034	8.680448	-0.054723	4.538334
270.381070	7085.145202	8.685453	-0.054774	4.540824
270.557968	7093.132849	8.690458	-0.054812	4.543301
270.577989	7101.135619	8.695463	-0.054821	4.545780
270.838010	7109.184248	8.700467	-0.054875	4.548273
271.216404	7117.185530	8.705472	-0.054950	4.550750
271.316640	7125.234644	8.710477	-0.054974	4.553239
271.434943	7133.301287	8.715482	-0.055001	4.555733
271.629052	7141.251911	8.720487	-0.055043	4.558190
271.959842	7149.283396	8.725491	-0.055110	4.560670
271.877811	7157.289055	8.730496	-0.055099	4.563141
272.277775	7165.287797	8.735501	-0.055179	4.565609
272.293858	7173.330329	8.740506	-0.055187	4.568088
272.453244	7181.283732	8.745511	-0.055222	4.570539
272.525232	7189.401841	8.750515	-0.055241	4.573039
272.605821	7197.390489	8.755520	-0.055261	4.575498
272.823274	7205.422884	8.760525	-0.055307	4.577969
272.993766	7213.429294	8.765530	-0.055343	4.580431
273.072982	7221.458463	8.770535	-0.055363	4.582898
273.025481	7229.478871	8.775539	-0.055360	4.585361
273.520573	7237.432079	8.780544	-0.055457	4.587803
273.810130	7245.447814	8.785549	-0.055516	4.590262
274.087378	7253.559633	8.790554	-0.055573	4.592749
273.842695	7261.613774	8.795559	-0.055533	4.595217
273.613525	7269.629340	8.800563	-0.055495	4.597673
273.908341	7277.497351	8.805568	-0.055555	4.600081
274.133813	7285.566546	8.810573	-0.055602	4.602550
274.477275	7293.465646	8.815578	-0.055671	4.604966
274.756163	7301.513033	8.820583	-0.055729	4.607425
274.943636	7309.578013	8.825587	-0.055769	4.609889
274.899161	7317.647057	8.830592	-0.055766	4.612352
275.119476	7325.655341	8.835597	-0.055812	4.614796
275.440478	7333.721392	8.840602	-0.055877	4.617256
275.361140	7341.653786	8.845607	-0.055867	4.619674
275.573557	7349.725239	8.850611	-0.055912	4.622133
275.899210	7357.652646	8.855616	-0.055978	4.624546
276.150172	7365.737026	8.860621	-0.056030	4.627006
276.150030	7373.752216	8.865626	-0.056035	4.629444
276.261916	7381.728832	8.870631	-0.056061	4.631869
276.566521	7389.786351	8.875635	-0.056123	4.634317
276.536660	7397.819355	8.880640	-0.056122	4.636757
276.790491	7405.787645	8.885645	-0.056175	4.639175
276.845175	7413.827384	8.890650	-0.056190	4.641614
276.991528	7421.754333	8.895655	-0.056222	4.644017
277.198054	7429.854704	8.900659	-0.056266	4.646472
277.374789	7437.813941	8.905664	-0.056304	4.648882
277.473239	7445.901846	8.910669	-0.056328	4.651330
277.695944	7453.900731	8.915674	-0.056374	4.653750
277.895648	7461.936804	8.920679	-0.056417	4.656180
278.017691	7469.952995	8.925683	-0.056445	4.658603
278.191241	7477.924072	8.930688	-0.056482	4.661011
278.400680	7485.948156	8.935693	-0.056526	4.663433
278.766525	7493.949462	8.940698	-0.056600	4.665847
278.750285	7501.975564	8.945703	-0.056602	4.668268
278.984566	7510.005304	8.950707	-0.056651	4.670688
279.138668	7518.106168	8.955712	-0.056684	4.673128
279.256831	7526.145769	8.960717	-0.056712	4.675549
279.627221	7534.083387	8.965722	-0.056786	4.677937
279.686481	7542.035510	8.970727	-0.056802	4.680329
279.702523	7550.097363	8.975731	-0.056810	4.682753
279.775604	7558.038087	8.980736	-0.056829	4.685140
280.041586	7566.060245	8.985741	-0.056884	4.687548
280.302982	7574.075162	8.990746	-0.056937	4.689954
280.399008	7582.122136	8.995751	-0.056961	4.692368
280.769401	7590.178650	9.000755	-0.057035	4.694783
280.878682	7598.188327	9.005760	-0.057060	4.697184
280.993639	7606.140699	9.010765	-0.057087	4.699566
281.015032	7614.193335	9.015770	-0.057096	4.701977
281.089123	7622.122244	9.020775	-0.057115	4.704350
281.450889	7630.218585	9.025779	-0.057187	4.706771
281.278159	7638.231755	9.030784	-0.057160	4.709167
281.530319	7646.250891	9.035789	-0.057213	4.711562
281.920748	7654.309013	9.040794	-0.057290	4.713968
281.710667	7662.297474	9.045799	-0.057257	4.716353
281.984339	7670.263383	9.050803	-0.057313	4.718729
282.130638	7678.317981	9.055808	-0.057345	4.721130
282.423610	7686.286080	9.060813	-0.057405	4.723504
282.469592	7694.334294	9.065818	-0.057419	4.725902
282.476126	7702.395632	9.070823	-0.057425	4.728302
282.669471	7710.422218	9.075827	-0.057466	4.730690
282.854089	7718.449695	9.080832	-0.057506	4.733077
283.129586	7726.440328	9.085837	-0.057562	4.735452
283.419175	7734.492003	9.090842	-0.057621	4.737843
283.421179	7742.447719	9.095847	-0.057627	4.740206
283.813027	7750.497324	9.100851	-0.057705	4.742594
284.047622	7758.445017	9.105856	-0.057754	4.744951
284.353365	7766.529282	9.110861	-0.057816	4.747347
284.357675	7774.507531	9.115866	-0.057822	4.749712
284.680269	7782.552884	9.120871	-0.057887	4.752094
284.754803	7790.602337	9.125875	-0.057906	4.754477
284.624006	7798.603554	9.130880	-0.057887	4.756845
284.728324	7806.579143	9.135885	-0.057912	4.759204
285.167781	7814.529501	9.140890	-0.057999	4.761552
285.083285	7822.550699	9.145895	-0.057988	4.763923
285.445240	7830.585295	9.150899	-0.058061	4.766294
285.622558	7838.670079	9.155904	-0.058099	4.768680
286.014903	7846.637195	9.160909	-0.058177	4.771029
286.159627	7854.663021	9.165914	-0.058209	4.773395
286.212926	7862.656577	9.170919	-0.058224	4.775751
286.410501	7870.679592	9.175923	-0.058266	4.778114
286.566105	7878.680572	9.180928	-0.058300	4.780469
286.759685	7886.707372	9.185933	-0.058342	4.782831
286.954303	7894.737175	9.190938	-0.058383	4.785192
286.872879	7902.726310	9.195943	-0.058373	4.787541
286.936537	7910.784360	9.200947	-0.058390	4.789909
286.989949	7918.820748	9.205952	-0.058405	4.792269
287.348381	7926.821445	9.210957	-0.058477	4.794616
287.621968	7934.879078	9.215962	-0.058533	4.796979
287.556116	7942.753034	9.220967	-0.058526	4.799289
287.844544	7950.896700	9.225971	-0.058585	4.801675
287.893958	7958.795300	9.230976	-0.058599	4.803989
287.985192	7966.848811	9.235981	-0.058622	4.806347
288.147076	7974.881956	9.240986	-0.058657	4.808697
288.459015	7982.887609	9.245991	-0.058720	4.811038
288.673007	7990.329551	9.250995	-0.058765	4.813213
288.530848	7994.810502	9.256000	-0.058741	4.814524

288.638535	7997.250159	9.261005	-0.058763	4.815236
288.734900	7998.605515	9.266010	-0.058782	4.815632
288.508512	7999.059756	9.271015	-0.058740	4.815766
288.696575	8000.054702	9.276019	-0.058775	4.816055
288.920963	8000.020309	9.281024	-0.058817	4.816044
288.947741	8000.059257	9.286029	-0.058822	4.816055
289.219961	8000.056720	9.291034	-0.058873	4.816053
289.122316	8000.037845	9.296039	-0.058854	4.816048
289.321922	8000.047879	9.301043	-0.058892	4.816050
289.354962	7999.989706	9.306048	-0.058898	4.816033
289.244919	7999.995182	9.311053	-0.058877	4.816035
289.313980	8000.042378	9.316058	-0.058890	4.816049
289.285970	7999.978823	9.321063	-0.058885	4.816030
289.430922	7999.997480	9.326067	-0.058912	4.816035
289.700600	7999.994897	9.331072	-0.058962	4.816033
289.730234	8000.003979	9.336077	-0.058967	4.816035
289.710095	8000.027116	9.341082	-0.058963	4.816042
289.874750	8000.030105	9.346087	-0.058994	4.816042
289.898809	8000.075416	9.351091	-0.058999	4.816055
289.794447	8000.037184	9.356096	-0.058979	4.816045
289.832599	8000.030394	9.361101	-0.058986	4.816042
290.008878	8000.043210	9.366106	-0.059019	4.816045
289.943325	8000.039877	9.371111	-0.059007	4.816045
290.026947	8000.058489	9.376115	-0.059022	4.816049
289.961962	8000.004945	9.381120	-0.059010	4.816034
289.917958	8000.065047	9.386125	-0.059002	4.816052
289.956840	8000.044379	9.391130	-0.059009	4.816046
290.116312	8000.038725	9.396135	-0.059039	4.816043
289.977053	8000.053286	9.401139	-0.059013	4.816048
290.083896	8000.046675	9.406144	-0.059032	4.816046
290.067028	8000.055981	9.411149	-0.059029	4.816049
290.066461	8000.041007	9.416154	-0.059029	4.816044
290.126966	8000.025006	9.421159	-0.059040	4.816039
290.249423	8000.063558	9.426163	-0.059063	4.816050
290.435208	8000.025258	9.431168	-0.059098	4.816038
290.280039	8000.049146	9.436173	-0.059069	4.816045
290.519906	8000.053502	9.441178	-0.059113	4.816045
290.492154	8000.050856	9.446183	-0.059108	4.816045
290.458565	8000.039555	9.451187	-0.059102	4.816042
290.551879	8000.020945	9.456192	-0.059119	4.816036
290.416336	8000.051601	9.461197	-0.059094	4.816045
290.511746	8000.062948	9.466202	-0.059112	4.816048
290.224816	8000.052385	9.471207	-0.059058	4.816047
290.421960	8000.092295	9.476211	-0.059095	4.816057
290.540296	8000.073071	9.481216	-0.059117	4.816051
290.433464	8000.104249	9.486221	-0.059097	4.816061
290.434739	8000.102131	9.491226	-0.059097	4.816060
290.635856	8000.076932	9.496231	-0.059134	4.816052
290.765966	8000.084636	9.501235	-0.059159	4.816053
290.626680	8000.039357	9.506240	-0.059133	4.816041
290.685502	8000.047902	9.511245	-0.059144	4.816043
290.708811	8000.060076	9.516250	-0.059148	4.816046
290.487698	8000.054982	9.521255	-0.059107	4.816046
290.748893	8000.081098	9.526259	-0.059155	4.816052
290.787479	8000.055081	9.531264	-0.059162	4.816045
290.762164	8000.082399	9.536269	-0.059158	4.816053
290.712800	8000.094320	9.541274	-0.059148	4.816056
290.750514	8000.077904	9.546279	-0.059155	4.816051
290.883595	8000.082457	9.551283	-0.059180	4.816052
290.789094	8000.033717	9.556288	-0.059162	4.816038
290.711034	8000.078241	9.561293	-0.059148	4.816052
290.959882	8000.076351	9.566298	-0.059194	4.816050
290.803718	8000.040381	9.571303	-0.059165	4.816040
290.920543	8000.071352	9.576307	-0.059187	4.816049
291.081359	8000.056107	9.581312	-0.059217	4.816043
291.015446	8000.005750	9.586317	-0.059204	4.816029
290.943576	8000.070689	9.591322	-0.059191	4.816048
291.037216	8000.048879	9.596327	-0.059208	4.816041
291.165732	8000.062966	9.601331	-0.059232	4.816045
290.961239	8000.054968	9.606336	-0.059194	4.816044
290.933873	8000.091866	9.611341	-0.059189	4.816054
291.010848	8000.108221	9.616346	-0.059203	4.816059
290.894328	8000.085795	9.621351	-0.059181	4.816053
290.979050	8000.081988	9.626355	-0.059197	4.816051
291.137785	8000.069911	9.631360	-0.059227	4.816047
291.081775	8000.079573	9.636365	-0.059216	4.816050
291.127475	8000.079332	9.641370	-0.059225	4.816050
291.182935	8000.045073	9.646375	-0.059235	4.816040
291.386246	8000.081892	9.651379	-0.059273	4.816049
291.276948	8000.061734	9.656384	-0.059252	4.816044
291.191025	8000.054824	9.661389	-0.059236	4.816042
291.323706	8000.076467	9.666394	-0.059261	4.816048
291.163519	8000.074617	9.671399	-0.059231	4.816048
291.222868	8000.074624	9.676403	-0.059242	4.816048
291.259845	8000.044303	9.681408	-0.059249	4.816039
291.382889	8000.042263	9.686413	-0.059272	4.816038
291.503235	8000.070093	9.691418	-0.059294	4.816045
291.609423	8000.048511	9.696423	-0.059314	4.816038
291.729260	8000.094498	9.701427	-0.059336	4.816051
291.591063	8000.067402	9.706432	-0.059310	4.816044
291.597588	8000.084614	9.711437	-0.059312	4.816049
291.615232	8000.106302	9.716442	-0.059315	4.816055
291.519287	8000.088523	9.721447	-0.059297	4.816050
291.569037	8000.099041	9.726451	-0.059306	4.816053
291.651457	8000.079164	9.731456	-0.059321	4.816047
291.563274	8000.074350	9.736461	-0.059305	4.816046
291.635579	8000.077798	9.741466	-0.059318	4.816047
291.551265	8000.082671	9.746471	-0.059303	4.816049
291.781446	8000.099677	9.751475	-0.059345	4.816052
291.575426	8000.071348	9.756480	-0.059307	4.816045
291.427466	8000.086818	9.761485	-0.059279	4.816050
291.480999	8000.086718	9.766490	-0.059289	4.816050
291.707235	8000.063046	9.771495	-0.059331	4.816042
291.716979	8000.096345	9.776499	-0.059333	4.816052
291.549562	8000.071923	9.781504	-0.059302	4.816045
291.548142	8000.091127	9.786509	-0.059302	4.816051
291.577492	8000.106617	9.791514	-0.059307	4.816055
291.245822	8000.064249	9.796519	-0.059245	4.816045
291.391683	8000.100023	9.801523	-0.059272	4.816054
291.472296	8000.065153	9.806528	-0.059287	4.816044
291.376542	8000.022801	9.811533	-0.059269	4.816032
291.468943	8000.085386	9.816538	-0.059287	4.816050
291.716769	8000.031118	9.821543	-0.059333	4.816033
291.554023	8000.079444	9.826547	-0.059302	4.816048
291.356386	8000.066228	9.831552	-0.059266	4.816045
291.593356	8000.052368	9.836557	-0.059310	4.816040
291.568127	8000.077550	9.841562	-0.059305	4.816047
291.567803	8000.052963	9.846567	-0.059305	4.816040
291.677745	8000.081673	9.851571	-0.059325	4.816048
291.885988	8000.064085	9.856576	-0.059364	4.816041
291.505985	8000.043277	9.861581	-0.059293	4.816037
291.865394	8000.062633	9.866586	-0.059360	4.816041
291.851153	8000.039929	9.871591	-0.059357	4.816035
291.878796	8000.063936	9.876595	-0.059362	4.816041
291.688143	8000.061532	9.881600	-0.059327	4.816042
291.671514	8000.054814	9.886605	-0.059324	4.816040
291.640933	8000.111956	9.891610	-0.059318	4.816057
291.606775	8000.053627	9.896615	-0.059312	4.816040
291.682298	8000.095602	9.901619	-0.059326	4.816052
291.882622	8000.080008	9.906624	-0.059363	4.816046
291.755421	8000.055249	9.911629	-0.059339	4.816040
291.982077	8000.091425	9.916634	-0.059381	4.816049
291.860092	8000.095613	9.921639	-0.059359	4.816051
291.653178	8000.083296	9.926643	-0.059320	4.816048
291.745048	8000.080688	9.931648	-0.059337	4.816047
291.747168	8000.076448	9.936653	-0.059337	4.816046
291.765938	8000.098157	9.941658	-0.059341	4.816052
291.645836	8000.058567	9.946663	-0.059318	4.816041
291.749966	8000.056183	9.951667	-0.059338	4.816040
291.952536	8000.042766	9.956672	-0.059375	4.816035
291.859038	8000.059226	9.961677	-0.059358	4.816040
291.927530	8000.074359	9.966682	-0.059371	4.816044
291.802304	8000.053911	9.971687	-0.059347	4.816039
291.835846	8000.091917	9.976691	-0.059353	4.816050
292.031653	8000.071966	9.981696	-0.059390	4.816043
291.973233	8000.081584	9.986701	-0.059379	4.816046
291.925100	8000.056127	9.991706	-0.059370	4.816039
291.882488	8000.077788	9.996711	-0.059362	4.816045
291.913234	8000.076205	10.001715	-0.059368	4.816045
292.077930	8000.089883	10.006720	-0.059398	4.816048
292.124765	8000.042644	10.011725	-0.059407	4.816034
291.962089	8000.100589	10.016730	-0.059377	4.816052
291.940842	8000.058524	10.021735	-0.059373	4.816040
292.089121	8000.062285	10.026739	-0.059400	4.816040
292.076365	8000.071666	10.031744	-0.059398	4.816043
292.144554	8000.076108	10.036749	-0.059410	4.816044
292.241742	8000.096038	10.041754	-0.059428	4.816049
291.996243	8000.059509	10.046759	-0.059383	4.816040
292.092743	8000.096524	10.051763	-0.059401	4.816050
292.208908	8000.068712	10.056768	-0.059422	4.816041
291.965712	8000.063215	10.061773	-0.059377	4.816041
291.932411	8000.096799	10.066778	-0.059371	4.816051
292.020841	8000.066346	10.071783	-0.059387	4.816041
292.001989	8000.058518	10.076787	-0.059383	4.816039
291.960829	8000.062040	10.081792	-0.059376	4.816040
292.092978	8000.085811	10.086797	-0.059400	4.816047
292.381177	8000.113490	10.091802	-0.059454	4.816053
292.187036	8000.074690	10.096807	-0.059418	4.816043
292.163529	8000.094561	10.101811	-0.059413	4.816049
292.206938	8000.090004	10.106816	-0.059421	4.816047
292.085399	8000.109160	10.111821	-0.059399	4.816054
292.150362	8000.114611	10.116826	-0.059411	4.816055
292.114557	8000.070143	10.121831	-0.059404	4.816042
292.358899	8000.113054	10.126835	-0.059450	4.816053
291.916888	8000.091116	10.131840	-0.059367	4.816049
291.913941	8000.082509	10.136845	-0.059367	4.816047
292.200816	8000.121919	10.141850	-0.059420	4.816057
292.141628	8000.073819	10.146855	-0.059409	4.816043
292.358460	8000.064937	10.151859	-0.059449	4.816039
292.465258	8000.056190	10.156864	-0.059469	4.816036
292.155758	8000.079406	10.161869	-0.059411	4.816045
292.243957	8000.100241	10.166874	-0.059428	4.816050
292.202871	8000.059951	10.171879	-0.059420	4.816039
292.329632	8000.081487	10.176883	-0.059444	4.816044
292.416420	8000.071308	10.181888	-0.059460	4.816041
292.220688	8000.052782	10.186893	-0.059423	4.816036
292.343384	8000.105233	10.191898	-0.059446	4.816051
292.324678	8000.078174	10.196903	-0.059442	4.816043
292.269442	8000.091056	10.201907	-0.059432	4.816047
292.264946	8000.083489	10.206912	-0.059431	4.816045
292.327641	8000.093174	10.211917	-0.059443	4.816048
292.189680	8000.103483	10.216922	-0.059417	4.816051
292.404730	8000.079608	10.221927	-0.059457	4.816043
292.282472	8000.079516	10.226931	-0.059434	4.816044
292.333311	8000.078299	10.231936	-0.059444	4.816043
292.312520	8000.047996	10.236941	-0.059440	4.816035
292.487445	8000.103536	10.241946	-0.059472	4.816050
292.406032	8000.088158	10.246951	-0.059457	4.816046
292.512830	8000.109332	10.251955	-0.059477	4.816051
292.646113	8000.101066	10.256960	-0.059502	4.816048
292.458813	8000.053841	10.261965	-0.059467	4.816035
292.361165	8000.073432	10.266970	-0.059449	4.816042
292.370598	8000.045816	10.271975	-0.059450	4.816034
292.543386	8000.098111	10.276979	-0.059482	4.816048
292.388921	8000.085678	10.281984	-0.059454	4.816045
292.341249	8000.100835	10.286989	-0.059445	4.816050
292.488634	8000.135570	10.291994	-0.059472	4.816059
292.374164	8000.058682	10.296999	-0.059451	4.816037
292.407645	8000.083864	10.302003	-0.059457	4.816045
292.193602	8000.072485	10.307008	-0.059417	4.816042
292.379372	8000.038460	10.312013	-0.059452	4.816031
292.340079	8000.107199	10.317018	-0.059444	4.816052
292.406995	8000.071011	10.322023	-0.059457	4.816041
292.591092	8000.043367	10.327027	-0.059491	4.816032
292.675597	8000.056655	10.332032	-0.059507	4.816035
292.469776	8000.061454	10.337037	-0.059468	4.816038
292.579692	8000.082684	10.342042	-0.059489	4.816043
292.585146	8000.053927	10.347047	-0.059490	4.816035
292.593756	8000.074382	10.352051	-0.059491	4.816041
292.445624	8000.094123	10.357056	-0.059464	4.816047
292.407959	8000.057101	10.362061	-0.059456	4.816037
292.403822	8000.074119	10.367066	-0.059456	4.816042
292.523056	8000.075215	10.372071	-0.059478	4.816041
292.391839	8000.097401	10.377075	-0.059453	4.816049
292.493387	8000.084284	10.382080	-0.059472	4.816044
292.331209	8000.089877	10.387085	-0.059442	4.816047
292.601478	8000.105477	10.392090	-0.059492	4.816050
292.474202	8000.072167	10.397095	-0.059468	4.816041
292.399229	8000.035535	10.402099	-0.059454	4.816030
292.401896	8000.084734	10.407104	-0.059455	4.816045
292.567570	8000.096293	10.412109	-0.059486	4.816047
292.510837	8000.095256	10.417114	-0.059475	4.816047
292.230127	8000.066635	10.422119	-0.059423	4.816040
292.623618	8000.064173	10.427123	-0.059496	4.816038
292.587334	8000.059234	10.432128	-0.059489	4.816036
292.612818	8000.041527	10.437133	-0.059494	4.816031
292.734646	8000.072591	10.442138	-0.059517	4.816040
292.755287	8000.053728	10.447143	-0.059520	4.816034
292.671175	8000.075702	10.452147	-0.059505	4.816041
292.356312	8000.081723	10.457152	-0.059446	4.816044
292.706972	8000.056041	10.462157	-0.059511	4.816035
292.730656	8000.088526	10.467162	-0.059516	4.816044
292.538198	8000.040138	10.472167	-0.059480	4.816031
292.810668	8000.063258	10.477171	-0.059530	4.816036
292.913066	8000.091832	10.482176	-0.059549	4.816044
292.842902	8000.080933	10.487181	-0.059536	4.816041
292.919305	8000.103691	10.492186	-0.059551	4.816048
292.884675	8000.105193	10.497191	-0.059544	4.816048
292.828563	8000.076384	10.502195	-0.059534	4.816040
293.008469	8000.093546	10.507200	-0.059567	4.816044
292.999542	8000.049566	10.512205	-0.059565	4.816031
293.021721	8000.070268	10.517210	-0.059569	4.816037
292.671549	8000.037177	10.522215	-0.059504	4.816030
292.750991	8000.045029	10.527219	-0.059519	4.816031
292.899764	8000.087270	10.532224	-0.059547	4.816043
292.631920	8000.050334	10.537229	-0.059497	4.816034
292.767572	8000.091268	10.542234	-0.059522	4.816045
292.883726	8000.066662	10.547239	-0.059543	4.816037
292.783515	8000.085137	10.552243	-0.059525	4.816043
292.724541	8000.095814	10.557248	-0.059514	4.816046
292.678687	8000.062917	10.562253	-0.059505	4.816037
292.832891	8000.080679	10.567258	-0.059534	4.816041
292.848491	8000.049969	10.572263	-0.059537	4.816032
292.941263	8000.126455	10.577267	-0.059554	4.816054
293.092233	8000.117444	10.582272	-0.059582	4.816051
292.906399	8000.085205	10.587277	-0.059547	4.816042
293.004370	8000.121179	10.592282	-0.059565	4.816052
292.870069	8000.088809	10.597287	-0.059540	4.816044
292.964633	8000.102280	10.602291	-0.059558	4.816047
293.087629	8000.121612	10.607296	-0.059581	4.816052
292.782855	8000.104306	10.612301	-0.059524	4.816049
292.979830	8000.102544	10.617306	-0.059561	4.816047
292.893608	8000.091353	10.622311	-0.059545	4.816044
292.756511	8000.116637	10.627315	-0.059519	4.816052
292.784480	8000.070123	10.632320	-0.059524	4.816039
292.597737	8000.028251	10.637325	-0.059489	4.816027
292.751492	8000.114395	10.642330	-0.059518	4.816052
292.656527	8000.063507	10.647335	-0.059500	4.816037
292.730946	8000.076611	10.652339	-0.059514	4.816041
292.591249	8000.051624	10.657344	-0.059488	4.816034
292.684126	8000.060790	10.662349	-0.059505	4.816036
292.960443	8000.114969	10.667354	-0.059557	4.816051
292.780077	8000.077487	10.672359	-0.059523	4.816041
292.838180	8000.096706	10.677363	-0.059534	4.816046
292.817939	8000.103814	10.682368	-0.059530	4.816048
292.825879	8000.061210	10.687373	-0.059531	4.816036
292.946296	8000.098661	10.692378	-0.059554	4.816046
293.034502	8000.102399	10.697383	-0.059570	4.816047
292.985689	8000.106849	10.702387	-0.059561	4.816048
292.987397	8000.100464	10.707392	-0.059561	4.816046
292.979840	8000.061852	10.712397	-0.059560	4.816035
292.912296	8000.110843	10.717402	-0.059547	4.816050
292.921302	8000.100316	10.722407	-0.059549	4.816047
292.854005	8000.101224	10.727411	-0.059536	4.816047
292.811288	8000.085482	10.732416	-0.059528	4.816043
292.903936	8000.062585	10.737421	-0.059545	4.816036
292.834734	8000.098723	10.742426	-0.059532	4.816047
292.803109	8000.072496	10.747431	-0.059527	4.816039
292.789193	8000.091473	10.752435	-0.059524	4.816045
292.905572	8000.085038	10.757440	-0.059546	4.816042
292.841127	8000.049666	10.762445	-0.059533	4.816032
293.042675	8000.081113	10.767450	-0.059571	4.816040
292.978738	8000.035063	10.772455	-0.059559	4.816027
292.925146	8000.080033	10.777459	-0.059549	4.816041
292.731053	8000.087183	10.782464	-0.059513	4.816044
292.990803	8000.039544	10.787469	-0.059561	4.816029
292.998989	8000.061060	10.792474	-0.059563	4.816035
292.926984	8000.052265	10.797479	-0.059549	4.816033
292.818079	8000.039593	10.802483	-0.059529	4.816030
292.741647	8000.068119	10.807488	-0.059515	4.816038
292.683972	8000.089505	10.812493	-0.059504	4.816045
292.962369	8000.080675	10.817498	-0.059556	4.816041
292.984261	8000.049011	10.822503	-0.059560	4.816031
292.983993	8000.060756	10.827507	-0.059559	4.816035
293.014814	8000.090165	10.832512	-0.059565	4.816043
293.023644	8000.062537	10.837517	-0.059567	4.816035
293.014051	8000.089074	10.842522	-0.059565	4.816043
293.018817	8000.069921	10.847527	-0.059566	4.816037
292.887645	8000.064323	10.852531	-0.059541	4.816036
292.948670	8000.101762	10.857536	-0.059553	4.816047
292.887421	8000.081408	10.862541	-0.059541	4.816041
292.918964	8000.114036	10.867546	-0.059547	4.816051
293.044919	8000.073579	10.872551	-0.059570	4.816038
293.053121	8000.075861	10.877555	-0.059572	4.816039
293.090191	8000.078669	10.882560	-0.059579	4.816040
293.108797	8000.042670	10.887565	-0.059582	4.816029
293.021680	8000.114814	10.892570	-0.059566	4.816050
292.902596	8000.098751	10.897575	-0.059544	4.816046
293.044094	8000.086361	10.902579	-0.059570	4.816042
292.951854	8000.087884	10.907584	-0.059553	4.816043
293.101098	8000.017930	10.912589	-0.059580	4.816022
292.980910	8000.100158	10.917594	-0.059558	4.816046
293.046359	8000.041503	10.922599	-0.059570	4.816029
293.043423	7999.969848	10.927603	-0.059570	4.816008
293.099883	8000.061703	10.932608	-0.059580	4.816035
293.115921	8000.033138	10.937613	-0.059583	4.816026
293.143231	8000.077443	10.942618	-0.059588	4.816039
293.163386	8000.055365	10.947623	-0.059592	4.816032
292.994850	8000.066185	10.952627	-0.059560	4.816036
292.983269	8000.091616	10.957632	-0.059558	4.816044
292.878137	8000.086493	10.962637	-0.059539	4.816043
293.117490	8000.117560	10.967642	-0.059583	4.816051
293.093073	8000.075435	10.972647	-0.059578	4.816039
293.154323	8000.093643	10.977651	-0.059590	4.816044
293.233192	8000.100417	10.982656	-0.059604	4.816045
293.085591	8000.065668	10.987661	-0.059577	4.816036
293.044431	8000.099110	10.992666	-0.059569	4.816046
293.074211	8000.059040	10.997671	-0.059575	4.816034
293.027063	8000.059246	11.002675	-0.059566	4.816034
293.055795	8000.116401	11.007680	-0.059571	4.816051
292.987806	8000.090581	11.012685	-0.059559	4.816044
292.996419	8000.117449	11.017690	-0.059560	4.816051
293.188487	8000.087813	11.022695	-0.059596	4.816042
293.114383	8000.072568	11.027699	-0.059582	4.816038
293.028793	8000.075280	11.032704	-0.059566	4.816039
292.959303	8000.029130	11.037709	-0.059553	4.816026
292.975371	8000.104220	11.042714	-0.059556	4.816048
293.046755	8000.078800	11.047719	-0.059569	4.816040
293.188156	8000.034350	11.052723	-0.059595	4.816026
293.180703	8000.063062	11.057728	-0.059594	4.816035
293.015973	8000.026933	11.062733	-0.059563	4.816025
293.003056	8000.067300	11.067738	-0.059561	4.816037
293.132062	8000.046134	11.072743	-0.059585	4.816030
293.171464	8000.063945	11.077747	-0.059592	4.816035
293.329402	8000.070021	11.082752	-0.059621	4.816036
293.278833	8000.029557	11.087757	-0.059612	4.816024
293.303827	8000.062066	11.092762	-0.059617	4.816034
292.938382	8000.073577	11.097767	-0.059549	4.816039
293.122636	8000.075857	11.102771	-0.059583	4.816039
293.218421	8000.092556	11.107776	-0.059601	4.816043
292.986526	8000.091537	11.112781	-0.059557	4.816044
292.978666	8000.079635	11.117786	-0.059556	4.816040
292.925028	8000.077586	11.122791	-0.059546	4.816040
292.989680	8000.074484	11.127795	-0.059558	4.816039
293.065252	8000.110050	11.132800	-0.059572	4.816049
293.001914	8000.065080	11.137805	-0.059560	4.816036
293.190944	8000.102711	11.142810	-0.059595	4.816046
292.977556	8000.113784	11.147815	-0.059555	4.816050
293.127328	8000.132534	11.152819	-0.059583	4.816055
293.204999	8000.144630	11.157824	-0.059598	4.816058
293.150898	8000.073112	11.162829	-0.059588	4.816038
293.192148	8000.079201	11.167834	-0.059595	4.816039
293.213718	8000.079589	11.172839	-0.059599	4.816039
293.068774	8000.049163	11.177843	-0.059572	4.816031
293.102891	8000.079701	11.182848	-0.059578	4.816040
292.931399	8000.037037	11.187853	-0.059546	4.816028
293.004546	8000.099274	11.192858	-0.059560	4.816046
292.865496	8000.068955	11.197863	-0.059534	4.816038
293.199539	8000.104951	11.202867	-0.059596	4.816047
293.210510	8000.131862	11.207872	-0.059598	4.816054
292.998690	8000.106630	11.212877	-0.059559	4.816048
293.167391	8000.106490	11.217882	-0.059590	4.816047
293.249946	8000.085547	11.222887	-0.059605	4.816041
293.328224	8000.111546	11.227891	-0.059620	4.816048
293.187232	8000.112181	11.232896	-0.059594	4.816049
293.282979	8000.079723	11.237901	-0.059611	4.816039
293.368173	8000.113328	11.242906	-0.059627	4.816048
293.279944	8000.076453	11.247911	-0.059611	4.816038
293.336804	8000.016573	11.252915	-0.059621	4.816020
293.438498	8000.066507	11.257920	-0.059640	4.816034
293.247766	8000.056619	11.262925	-0.059605	4.816032
293.201958	8000.040821	11.267930	-0.059596	4.816028
293.217116	8000.076356	11.272935	-0.059599	4.816038
293.181480	8000.058605	11.277939	-0.059592	4.816033
293.318928	8000.102778	11.282944	-0.059618	4.816045
293.228421	8000.043422	11.287949	-0.059601	4.816029
293.423360	8000.106808	11.292954	-0.059637	4.816046
293.317715	8000.120909	11.297959	-0.059617	4.816051
293.105752	8000.061479	11.302963	-0.059578	4.816035
293.553545	8000.076037	11.307968	-0.059661	4.816036
293.225045	8000.063641	11.312973	-0.059600	4.816035
293.189472	8000.065127	11.317978	-0.059593	4.816035
293.280866	8000.063580	11.322983	-0.059610	4.816034
293.236716	8000.045674	11.327987	-0.059602	4.816029
293.169973	8000.067964	11.332992	-0.059590	4.816036
293.242955	8000.079974	11.337997	-0.059603	4.816039
293.365962	8000.133502	11.343002	-0.059626	4.816054
293.241664	8000.087422	11.348007	-0.059603	4.816041
293.423943	8000.047991	11.353011	-0.059637	4.816029
293.471840	8000.086260	11.358016	-0.059645	4.816040
293.249694	8000.069388	11.363021	-0.059604	4.816036
293.213178	8000.063376	11.368026	-0.059597	4.816035
293.166090	8000.076407	11.373031	-0.059588	4.816039
293.432823	8000.069502	11.378035	-0.059638	4.816035
293.254489	8000.095105	11.383040	-0.059605	4.816044
293.254409	8000.068383	11.388045	-0.059605	4.816036
293.389567	8000.093280	11.393050	-0.059630	4.816042
293.350768	8000.073334	11.398055	-0.059623	4.816037
293.395675	8000.067735	11.403059	-0.059631	4.816035
293.382803	8000.087800	11.408064	-0.059628	4.816041
293.359805	8000.052113	11.413069	-0.059624	4.816030
293.231234	8000.081827	11.418074	-0.059600	4.816040
293.382233	8000.101668	11.423079	-0.059628	4.816045
293.324894	8000.049327	11.428083	-0.059617	4.816030
293.445405	8000.104947	11.433088	-0.059640	4.816045
293.441683	8000.070679	11.438093	-0.059639	4.816035
293.311469	8000.120666	11.443098	-0.059615	4.816051
293.237451	8000.065884	11.448103	-0.059601	4.816035
293.287122	8000.083881	11.453107	-0.059610	4.816040
293.433885	8000.086548	11.458112	-0.059638	4.816040
293.460327	8000.064584	11.463117	-0.059642	4.816034
293.283820	8000.054955	11.468122	-0.059609	4.816032
293.377542	8000.076960	11.473127	-0.059627	4.816038
293.411039	8000.060468	11.478131	-0.059633	4.816033
293.237802	8000.081888	11.483136	-0.059601	4.816040
293.312349	8000.028741	11.488141	-0.059615	4.816024
293.425536	8000.073541	11.493146	-0.059636	4.816036
293.390857	8000.081455	11.498151	-0.059629	4.816039
293.321812	8000.072713	11.503155	-0.059616	4.816037
293.503877	8000.101669	11.508160	-0.059650	4.816044
293.332003	8000.085713	11.513165	-0.059618	4.816040
293.346077	8000.116955	11.518170	-0.059621	4.816049
293.424193	8000.091657	11.523175	-0.059635	4.816042
293.367970	8000.035061	11.528179	-0.059625	4.816025
293.578342	8000.037817	11.533184	-0.059664	4.816025
293.278292	8000.055861	11.538189	-0.059608	4.816032
293.511598	8000.100710	11.543194	-0.059651	4.816044
293.459468	8000.071973	11.548199	-0.059641	4.816036
293.214288	7999.974537	11.553203	-0.059596	4.816009
293.552699	8000.027710	11.558208	-0.059659	4.816022
293.467405	8000.073172	11.563213	-0.059643	4.816036
293.429074	8000.054304	11.568218	-0.059636	4.816031
293.455894	8000.088983	11.573223	-0.059641	4.816041
293.399958	8000.024912	11.578227	-0.059630	4.816022
293.518422	8000.096524	11.583232	-0.059652	4.816043
293.316717	8000.055447	11.588237	-0.059614	4.816032
293.278681	8000.026966	11.593242	-0.059607	4.816024
293.468359	8000.044306	11.598247	-0.059643	4.816028
293.377904	8000.022351	11.603251	-0.059626	4.816022
293.394619	8000.099591	11.608256	-0.059629	4.816044
293.368204	8000.067048	11.613261	-0.059624	4.816035
293.288074	8000.074134	11.618266	-0.059609	4.816037
293.231069	8000.083778	11.623271	-0.059598	4.816040
293.340891	8000.071880	11.628275	-0.059619	4.816036
293.441784	8000.081192	11.633280	-0.059637	4.816039
293.406012	8000.057027	11.638285	-0.059631	4.816032
293.559677	8000.094016	11.643290	-0.059659	4.816042
293.634227	8000.069721	11.648295	-0.059673	4.816034
293.304297	8000.039133	11.653299	-0.059612	4.816027
293.437434	8000.065062	11.658304	-0.059636	4.816034
293.620398	8000.032054	11.663309	-0.059670	4.816023
293.530497	8000.068884	11.668314	-0.059654	4.816035
293.417621	8000.060413	11.673319	-0.059633	4.816033
293.382362	8000.084345	11.678323	-0.059626	4.816040
293.429859	8000.087342	11.683328	-0.059635	4.816040
293.285472	8000.047308	11.688333	-0.059608	4.816030
293.379225	8000.068245	11.693338	-0.059625	4.816035
293.546276	8000.060595	11.698343	-0.059656	4.816032
293.500789	8000.027704	11.703347	-0.059648	4.816023
293.426573	8000.119319	11.708352	-0.059634	4.816050
293.436170	8000.089568	11.713357	-0.059636	4.816041
293.636535	8000.114583	11.718362	-0.059673	4.816047
293.537892	8000.081793	11.723367	-0.059654	4.816038
293.410582	8000.073059	11.728371	-0.059631	4.816036
293.545287	8000.055203	11.733376	-0.059656	4.816030
293.607679	8000.061677	11.738381	-0.059667	4.816032
293.611483	8000.115173	11.743386	-0.059668	4.816048
293.692994	8000.100623	11.748391	-0.059683	4.816043
293.411431	8000.121140	11.753395	-0.059631	4.816050
293.451360	8000.093010	11.758400	-0.059638	4.816042
293.542332	8000.092524	11.763405	-0.059655	4.816041
293.382018	8000.112042	11.768410	-0.059625	4.816048
293.201694	8000.115168	11.773415	-0.059591	4.816050
293.339195	8000.062098	11.778419	-0.059617	4.816034
293.699917	8000.095375	11.783424	-0.059684	4.816041
293.427134	8000.077581	11.788429	-0.059633	4.816038
293.313637	8000.104364	11.793434	-0.059612	4.816046
293.438354	8000.088463	11.798439	-0.059635	4.816041
293.355653	8000.051689	11.803443	-0.059620	4.816030
293.522460	8000.113495	11.808448	-0.059651	4.816048
293.528993	8000.091168	11.813453	-0.059652	4.816041
293.608004	8000.079778	11.818458	-0.059667	4.816037
293.329169	8000.061875	11.823463	-0.059615	4.816034
293.149997	8000.087462	11.828467	-0.059581	4.816042
293.684621	8000.151689	11.833472	-0.059681	4.816058
293.598107	8000.119119	11.838477	-0.059665	4.816049
293.429286	8000.113905	11.843482	-0.059633	4.816048
293.538727	8000.121235	11.848487	-0.059653	4.816050
293.564525	8000.088573	11.853491	-0.059658	4.816040
293.545400	8000.106387	11.858496	-0.059655	4.816045
293.499172	8000.083100	11.863501	-0.059646	4.816039
293.653098	8000.045290	11.868506	-0.059675	4.816027
293.639654	8000.086717	11.873511	-0.059672	4.816039
293.424189	8000.092408	11.878515	-0.059632	4.816042
293.626264	8000.130278	11.883520	-0.059669	4.816052
293.596930	8000.056005	11.888525	-0.059664	4.816030
293.417286	8000.081583	11.893530	-0.059630	4.816039
293.754529	8000.086649	11.898535	-0.059693	4.816039
293.672491	8000.062710	11.903539	-0.059678	4.816032
293.814427	8000.112308	11.908544	-0.059704	4.816046
293.564782	8000.062877	11.913549	-0.059658	4.816033
293.582411	8000.081360	11.918554	-0.059661	4.816038
293.600163	8000.094502	11.923559	-0.059664	4.816042
293.566959	8000.077864	11.928563	-0.059658	4.816037
293.756879	8000.100552	11.933568	-0.059693	4.816043
293.756013	8000.058856	11.938573	-0.059693	4.816030
293.506679	8000.137665	11.943578	-0.059647	4.816055
293.583269	8000.121957	11.948583	-0.059661	4.816050
293.506534	8000.094909	11.953587	-0.059647	4.816042
293.731820	8000.118240	11.958592	-0.059688	4.816048
293.617982	8000.062732	11.963597	-0.059667	4.816032
293.854069	8000.076643	11.968602	-0.059711	4.816035
293.819618	8000.109139	11.973607	-0.059705	4.816045
293.647392	8000.096382	11.978611	-0.059673	4.816042
293.617646	8000.147130	11.983616	-0.059667	4.816057
293.766580	8000.106023	11.988621	-0.059695	4.816044
293.808725	8000.133501	11.993626	-0.059702	4.816052
293.899461	8000.125531	11.998631	-0.059719	4.816049
293.735207	8000.133223	12.003635	-0.059689	4.816052
293.596703	8000.126422	12.008640	-0.059663	4.816051
293.712730	8000.123187	12.013645	-0.059684	4.816049
293.810910	8000.099323	12.018650	-0.059703	4.816042
293.692069	8000.126008	12.023655	-0.059680	4.816050
293.625921	8000.105564	12.028659	-0.059668	4.816045
293.764709	8000.096331	12.033664	-0.059694	4.816041
293.694452	8000.082224	12.038669	-0.059681	4.816038
293.827046	8000.113486	12.043674	-0.059705	4.816046
293.844383	8000.118072	12.048679	-0.059709	4.816047
294.007444	8000.067604	12.053683	-0.059739	4.816032
294.033756	8000.127922	12.058688	-0.059744	4.816049
293.986937	8000.086458	12.063693	-0.059735	4.816037
293.874955	8000.076934	12.068698	-0.059714	4.816035
293.808137	8000.075713	12.073703	-0.059702	4.816035
293.798607	8000.016761	12.078707	-0.059700	4.816018
293.858978	8000.099071	12.083712	-0.059711	4.816042
293.854594	8000.059448	12.088717	-0.059710	4.816030
293.787334	8000.049670	12.093722	-0.059698	4.816028
293.727335	8000.098798	12.098727	-0.059686	4.816042
293.696694	8000.083275	12.103731	-0.059681	4.816038
293.745621	8000.089505	12.108736	-0.059690	4.816040
293.627958	8000.093770	12.113741	-0.059668	4.816041
293.825599	8000.111256	12.118746	-0.059704	4.816045
293.760881	8000.109004	12.123751	-0.059692	4.816045
293.559131	8000.080749	12.128755	-0.059655	4.816038
293.894054	8000.112488	12.133760	-0.059717	4.816045
293.886025	8000.081348	12.138765	-0.059715	4.816036
293.714966	8000.101739	12.143770	-0.059684	4.816043
293.769297	8000.120890	12.148775	-0.059694	4.816049
293.745553	8000.058473	12.153779	-0.059689	4.816030
293.802148	8000.134303	12.158784	-0.059700	4.816052
293.638537	8000.100330	12.163789	-0.059669	4.816043
293.840796	8000.123243	12.168794	-0.059707	4.816049
293.861093	8000.120402	12.173799	-0.059711	4.816048
293.669200	8000.037826	12.178803	-0.059675	4.816025
293.619743	8000.091421	12.183808	-0.059666	4.816041
293.598526	8000.115608	12.188813	-0.059662	4.816048
293.518048	8000.124825	12.193818	-0.059646	4.816051
293.616681	8000.128753	12.198823	-0.059665	4.816052
293.746259	8000.101186	12.203827	-0.059689	4.816043
293.837317	8000.091085	12.208832	-0.059706	4.816040
293.581879	8000.065058	12.213837	-0.059658	4.816033
293.653061	8000.059937	12.218842	-0.059671	4.816031
293.677868	8000.071071	12.223847	-0.059676	4.816035
293.559064	8000.064629	12.228851	-0.059654	4.816033
293.605195	8000.113552	12.233856	-0.059662	4.816047
293.709411	8000.094073	12.238861	-0.059682	4.816041
293.790765	8000.094480	12.243866	-0.059697	4.816041
293.778582	8000.119901	12.248871	-0.059695	4.816048
293.628447	8000.082968	12.253875	-0.059666	4.816038
293.521077	8000.148332	12.258880	-0.059646	4.816058
293.500047	8000.126572	12.263885	-0.059643	4.816052
293.445268	8000.106335	12.268890	-0.059632	4.816046
293.825369	8000.127142	12.273895	-0.059703	4.816050
293.658651	8000.089907	12.278899	-0.059672	4.816040
293.705845	8000.119614	12.283904	-0.059681	4.816049
293.733279	8000.098737	12.288909	-0.059686	4.816042
293.774765	8000.104831	12.293914	-0.059693	4.816044
293.742459	8000.123473	12.298919	-0.059687	4.816049
293.827361	8000.105779	12.303923	-0.059703	4.816044
293.925185	8000.123585	12.308928	-0.059721	4.816049
293.703878	8000.054366	12.313933	-0.059680	4.816030
293.746427	8000.071165	12.318938	-0.059688	4.816034
294.005795	8000.102598	12.323943	-0.059736	4.816042
293.684461	8000.041175	12.328947	-0.059676	4.816026
293.749423	8000.121432	12.333952	-0.059688	4.816049
293.884731	8000.066185	12.338957	-0.059713	4.816032
293.814504	8000.088411	12.343962	-0.059700	4.816039
293.837960	8000.118756	12.348967	-0.059705	4.816048
293.873342	8000.109778	12.353971	-0.059711	4.816045
293.923934	8000.156645	12.358976	-0.059721	4.816058
293.694045	8000.091544	12.363981	-0.059678	4.816040
293.679658	8000.073111	12.368986	-0.059675	4.816035
293.969732	8000.126475	12.373991	-0.059729	4.816049
293.880074	8000.093848	12.378995	-0.059712	4.816040
293.876663	8000.120498	12.384000	-0.059712	4.816048
293.877357	8000.096996	12.389005	-0.059712	4.816041
293.987408	8000.049838	12.394010	-0.059732	4.816027
293.893379	8000.090867	12.399015	-0.059714	4.816039
293.910124	8000.077275	12.404019	-0.059718	4.816035
293.914307	8000.120092	12.409024	-0.059718	4.816048
293.701970	8000.085232	12.414029	-0.059679	4.816039
293.613828	8000.121025	12.419034	-0.059662	4.816049
293.821113	8000.085254	12.424039	-0.059701	4.816038
293.831208	8000.055512	12.429043	-0.059703	4.816029
293.873967	8000.117198	12.434048	-0.059711	4.816047
293.798803	8000.090178	12.439053	-0.059697	4.816040
294.020208	8000.114508	12.444058	-0.059738	4.816045
294.041572	8000.106344	12.449063	-0.059742	4.816043
294.039901	8000.062495	12.454067	-0.059741	4.816030
294.184782	8000.123903	12.459072	-0.059768	4.816047
294.023914	8000.062195	12.464077	-0.059738	4.816030
293.944611	8000.117384	12.469082	-0.059723	4.816047
293.991457	8000.126782	12.474087	-0.059732	4.816049
293.904243	8000.114503	12.479091	-0.059716	4.816046
293.880997	8000.082016	12.484096	-0.059711	4.816037
294.023614	8000.086746	12.489101	-0.059738	4.816037
293.983281	8000.078526	12.494106	-0.059730	4.816035
294.129767	8000.107905	12.499111	-0.059758	4.816043
293.866833	8000.082809	12.504115	-0.059709	4.816037
293.909263	8000.111362	12.509120	-0.059716	4.816045
294.054866	8000.101184	12.514125	-0.059744	4.816041
293.886764	8000.100257	12.519130	-0.059712	4.816042
294.154851	8000.117957	12.524135	-0.059762	4.816046
294.097958	8000.073103	12.529139	-0.059751	4.816033
294.094891	8000.121131	12.534144	-0.059751	4.816047
293.971114	8000.083608	12.539149	-0.059728	4.816037
294.033551	8000.099701	12.544154	-0.059739	4.816041
294.248339	8000.120705	12.549159	-0.059779	4.816046
293.917515	8000.061246	12.554163	-0.059718	4.816030
294.039859	8000.109420	12.559168	-0.059740	4.816044
294.081690	8000.114452	12.564173	-0.059748	4.816045
293.992952	8000.118175	12.569178	-0.059731	4.816047
293.967338	8000.081371	12.574183	-0.059727	4.816036
294.024314	8000.078129	12.579187	-0.059737	4.816035
293.937758	8000.057313	12.584192	-0.059721	4.816029
293.871524	8000.016564	12.589197	-0.059709	4.816018
294.068652	8000.060756	12.594202	-0.059745	4.816030
294.203231	8000.139075	12.599207	-0.059770	4.816052
293.886455	8000.085215	12.604211	-0.059711	4.816038
294.001240	8000.122565	12.609216	-0.059733	4.816048
294.075453	8000.104676	12.614221	-0.059746	4.816042
294.027212	8000.117685	12.619226	-0.059737	4.816046
294.056225	8000.132101	12.624231	-0.059743	4.816050
293.921588	8000.091175	12.629235	-0.059718	4.816039
293.997897	8000.080805	12.634240	-0.059732	4.816036
294.076796	8000.093992	12.639245	-0.059746	4.816039
294.010363	8000.057513	12.644250	-0.059734	4.816029
293.985277	8000.101934	12.649255	-0.059729	4.816042
293.923754	8000.054859	12.654259	-0.059718	4.816029
293.900228	8000.102514	12.659264	-0.059713	4.816043
293.830532	8000.100172	12.664269	-0.059700	4.816042
293.823663	8000.081876	12.669274	-0.059699	4.816037
293.989355	8000.110535	12.674279	-0.059730	4.816045
294.013447	8000.078910	12.679283	-0.059734	4.816035
294.164083	8000.120119	12.684288	-0.059762	4.816046
294.007785	8000.085210	12.689293	-0.059733	4.816037
293.955252	8000.097073	12.694298	-0.059723	4.816041
294.018103	8000.136683	12.699303	-0.059735	4.816052
293.829201	8000.090495	12.704307	-0.059700	4.816040
293.841100	8000.136658	12.709312	-0.059702	4.816053
293.842188	8000.113163	12.714317	-0.059702	4.816046
293.823298	8000.116021	12.719322	-0.059699	4.816047
294.062495	8000.117165	12.724327	-0.059743	4.816046
294.009314	8000.059555	12.729331	-0.059733	4.816030
294.035651	8000.112393	12.734336	-0.059738	4.816045
293.907694	8000.086549	12.739341	-0.059714	4.816038
293.896240	8000.105572	12.744346	-0.059712	4.816044
294.161794	8000.136049	12.749351	-0.059761	4.816051
294.042530	8000.126393	12.754355	-0.059739	4.816049
293.992074	8000.121195	12.759360	-0.059730	4.816048
294.081878	8000.117482	12.764365	-0.059746	4.816046
293.922051	8000.095333	12.769370	-0.059716	4.816040
293.941251	8000.113845	12.774375	-0.059720	4.816046
294.059756	8000.091419	12.779379	-0.059742	4.816039
294.170910	8000.118017	12.784384	-0.059763	4.816046
294.068128	8000.107592	12.789389	-0.059743	4.816043
294.246780	8000.101223	12.794394	-0.059777	4.816040
293.995957	8000.134054	12.799399	-0.059730	4.816051
293.854459	8000.091934	12.804403	-0.059704	4.816040
294.067856	8000.113981	12.809408	-0.059743	4.816045
294.172143	8000.119081	12.814413	-0.059763	4.816046
294.031809	8000.111179	12.819418	-0.059736	4.816045
294.133331	8000.113022	12.824423	-0.059755	4.816045
293.961214	8000.084237	12.829427	-0.059723	4.816037
293.837496	8000.096941	12.834432	-0.059700	4.816041
293.746929	8000.107043	12.839437	-0.059683	4.816045
293.829582	8000.080759	12.844442	-0.059699	4.816037
294.067483	8000.129968	12.849447	-0.059743	4.816050
293.887840	8000.088222	12.854451	-0.059709	4.816039
293.943592	8000.120223	12.859456	-0.059720	4.816048
293.897750	8000.091600	12.864461	-0.059711	4.816040
294.026647	8000.108903	12.869466	-0.059735	4.816044
294.065432	8000.130977	12.874471	-0.059742	4.816050
294.095927	8000.133665	12.879475	-0.059748	4.816051
294.255058	8000.128009	12.884480	-0.059777	4.816048
293.944510	8000.098840	12.889485	-0.059720	4.816041
293.976091	8000.105823	12.894490	-0.059725	4.816043
294.268466	8000.122896	12.899495	-0.059780	4.816047
293.845534	8000.099162	12.904499	-0.059701	4.816042
294.016380	8000.122572	12.909504	-0.059733	4.816048
294.137687	8000.115159	12.914509	-0.059755	4.816045
294.029842	8000.099298	12.919514	-0.059735	4.816041
293.929162	8000.131657	12.924519	-0.059716	4.816051
293.918472	8000.082301	12.929523	-0.059714	4.816037
294.083536	8000.133390	12.934528	-0.059745	4.816051
294.036309	8000.126114	12.939533	-0.059736	4.816049
294.020320	8000.101240	12.944538	-0.059733	4.816042
294.023211	8000.123729	12.949543	-0.059734	4.816048
293.997021	8000.079434	12.954547	-0.059729	4.816035
294.041235	8000.099470	12.959552	-0.059737	4.816041
294.127619	8000.077528	12.964557	-0.059753	4.816034
294.323969	8000.082167	12.969562	-0.059789	4.816035
294.215131	8000.095142	12.974567	-0.059769	4.816039
294.189681	8000.063684	12.979571	-0.059764	4.816030
294.332923	8000.121857	12.984576	-0.059791	4.816046
294.249193	8000.109641	12.989581	-0.059775	4.816043
294.161298	8000.119792	12.994586	-0.059759	4.816046
294.211875	8000.126051	12.999591	-0.059768	4.816048
293.944165	8000.103006	13.004595	-0.059718	4.816043
293.792159	8000.099166	13.009600	-0.059690	4.816042
294.037636	8000.110042	13.014605	-0.059736	4.816044
294.125778	8000.094544	13.019610	-0.059752	4.816039
294.184742	8000.122329	13.024615	-0.059763	4.816047
294.200480	8000.082003	13.029619	-0.059766	4.816035
294.376251	8000.127944	13.034624	-0.059799	4.816048
294.362327	8000.126618	13.039629	-0.059796	4.816047
294.230766	8000.104982	13.044634	-0.059771	4.816042
294.278551	8000.115465	13.049639	-0.059780	4.816045
294.214270	8000.070477	13.054643	-0.059768	4.816032
294.066115	8000.111589	13.059648	-0.059741	4.816045
294.184264	8000.108392	13.064653	-0.059763	4.816043
294.153882	8000.086462	13.069658	-0.059757	4.816037
293.984190	8000.120770	13.074663	-0.059725	4.816048
294.018872	8000.102162	13.079667	-0.059732	4.816042
293.978449	8000.074706	13.084672	-0.059724	4.816034
294.096520	8000.101429	13.089677	-0.059746	4.816041
294.105429	8000.096244	13.094682	-0.059748	4.816040
294.208447	8000.119488	13.099687	-0.059767	4.816046
294.209407	8000.072481	13.104691	-0.059767	4.816032
294.171080	8000.149789	13.109696	-0.059760	4.816055
294.054099	8000.146586	13.114701	-0.059738	4.816055
294.158626	8000.105739	13.119706	-0.059757	4.816042
294.419184	8000.126508	13.124711	-0.059806	4.816047
294.234873	8000.100706	13.129715	-0.059771	4.816040
294.269414	8000.130184	13.134720	-0.059778	4.816049
294.132729	8000.075328	13.139725	-0.059752	4.816034
293.993099	8000.105909	13.144730	-0.059726	4.816043
294.283379	8000.167827	13.149735	-0.059780	4.816060
293.952226	8000.120117	13.154739	-0.059719	4.816048
293.844706	8000.153420	13.159744	-0.059699	4.816058
293.612770	8000.149193	13.164749	-0.059655	4.816058
293.725799	8000.089266	13.169754	-0.059676	4.816040
293.683501	8000.170775	13.174759	-0.059668	4.816064
293.835448	8000.092321	13.179763	-0.059697	4.816040
294.137437	8000.139491	13.184768	-0.059753	4.816052
294.301670	8000.121105	13.189773	-0.059783	4.816046
294.157662	8000.115272	13.194778	-0.059756	4.816045
294.185503	8000.112569	13.199783	-0.059762	4.816044
294.239321	8000.076142	13.204787	-0.059772	4.816033
294.310567	8000.105219	13.209792	-0.059785	4.816041
294.353793	8000.085698	13.214797	-0.059793	4.816035
294.403157	8000.064150	13.219802	-0.059802	4.816029
294.394649	8000.087501	13.224807	-0.059800	4.816036
294.341768	8000.086534	13.229811	-0.059790	4.816036
294.351968	8000.094196	13.234816	-0.059792	4.816038
294.298020	8000.120993	13.239821	-0.059782	4.816046
294.208186	8000.093706	13.244826	-0.059765	4.816039
294.364563	8000.126471	13.249831	-0.059794	4.816047
294.407895	8000.121912	13.254835	-0.059802	4.816046
294.290330	8000.113355	13.259840	-0.059781	4.816044
294.208464	8000.130027	13.264845	-0.059765	4.816049
294.286120	8000.116475	13.269850	-0.059780	4.816045
294.390812	8000.155780	13.274855	-0.059799	4.816056
294.202808	8000.114950	13.279859	-0.059764	4.816045
294.205160	8000.126743	13.284864	-0.059764	4.816048
294.341924	8000.127091	13.289869	-0.059790	4.816048
294.397800	8000.101388	13.294874	-0.059800	4.816040
294.382720	8000.116070	13.299879	-0.059797	4.816044
294.263913	8000.088255	13.304883	-0.059775	4.816037
294.259214	8000.086028	13.309888	-0.059774	4.816036
294.377667	8000.101004	13.314893	-0.059796	4.816040
294.207899	8000.089359	13.319898	-0.059765	4.816037
294.301349	8000.129527	13.324903	-0.059782	4.816049
294.035387	8000.093690	13.329907	-0.059732	4.816040
294.297592	8000.108077	13.334912	-0.059781	4.816042
294.139998	8000.113752	13.339917	-0.059752	4.816045
294.078584	8000.103012	13.344922	-0.059740	4.816042
294.456181	8000.113089	13.349927	-0.059811	4.816043
294.492237	8000.091299	13.354931	-0.059817	4.816036
294.476312	8000.115584	13.359936	-0.059814	4.816044
294.487350	8000.115780	13.364941	-0.059816	4.816044
294.192513	8000.066593	13.369946	-0.059761	4.816031
294.243138	8000.133766	13.374951	-0.059771	4.816050
294.175598	8000.069482	13.379955	-0.059758	4.816032
294.273725	8000.090500	13.384960	-0.059776	4.816037
294.493330	8000.120141	13.389965	-0.059817	4.816045
294.330756	8000.111833	13.394970	-0.059787	4.816043
294.551551	8000.130810	13.399975	-0.059828	4.816048
294.670096	8000.111592	13.404979	-0.059850	4.816041
294.441679	8000.127732	13.409984	-0.059807	4.816047
294.503303	8000.113889	13.414989	-0.059819	4.816043
294.472890	8000.093026	13.419994	-0.059813	4.816037
294.616027	8000.136237	13.424999	-0.059840	4.816049
294.474294	8000.101592	13.430003	-0.059813	4.816040
294.430219	8000.137119	13.435008	-0.059805	4.816050
294.443574	8000.111710	13.440013	-0.059807	4.816043
294.442629	8000.107414	13.445018	-0.059807	4.816041
294.668959	8000.131835	13.450023	-0.059849	4.816047
294.422985	8000.096361	13.455027	-0.059803	4.816038
294.475336	8000.112270	13.460032	-0.059813	4.816043
294.363546	8000.123054	13.465037	-0.059792	4.816046
294.372896	8000.111465	13.470042	-0.059794	4.816043
294.516063	8000.116205	13.475047	-0.059821	4.816044
294.443568	8000.097782	13.480051	-0.059807	4.816039
294.465470	8000.092833	13.485056	-0.059811	4.816037
294.542214	8000.108118	13.490061	-0.059825	4.816041
294.412527	8000.082242	13.495066	-0.059801	4.816034
294.300183	8000.086604	13.500071	-0.059780	4.816036
294.265643	8000.069941	13.505075	-0.059774	4.816031
294.339965	8000.118310	13.510080	-0.059788	4.816045
294.381526	8000.117994	13.515085	-0.059795	4.816045
294.276585	8000.095774	13.520090	-0.059776	4.816039
294.534317	8000.122904	13.525095	-0.059824	4.816045
294.357267	8000.096166	13.530099	-0.059791	4.816039
294.428116	8000.126305	13.535104	-0.059804	4.816047
294.489441	8000.138103	13.540109	-0.059815	4.816050
294.597691	8000.118697	13.545114	-0.059835	4.816044
294.537946	8000.147527	13.550119	-0.059824	4.816053
294.427556	8000.102766	13.555123	-0.059803	4.816040
294.299699	8000.152797	13.560128	-0.059780	4.816055
294.411730	8000.146284	13.565133	-0.059800	4.816053
294.105358	8000.091544	13.570138	-0.059743	4.816039
294.426827	8000.097392	13.575143	-0.059803	4.816039
294.232465	8000.106672	13.580147	-0.059767	4.816042
294.330973	8000.078540	13.585152	-0.059785	4.816034
294.616789	8000.143584	13.590157	-0.059838	4.816051
294.534657	8000.093994	13.595162	-0.059823	4.816037
294.441025	8000.126482	13.600167	-0.059806	4.816047
294.427569	8000.081349	13.605171	-0.059803	4.816034
294.591996	8000.119604	13.610176	-0.059834	4.816044
294.604550	8000.120897	13.615181	-0.059836	4.816045
294.363233	8000.125047	13.620186	-0.059791	4.816047
294.383769	8000.121142	13.625191	-0.059795	4.816046
294.402640	8000.084079	13.630195	-0.059798	4.816035
294.476375	8000.075799	13.635200	-0.059812	4.816032
294.409998	8000.105577	13.640205	-0.059799	4.816041
294.529188	8000.097056	13.645210	-0.059822	4.816038
294.386740	8000.101938	13.650215	-0.059795	4.816040
294.296333	8000.096013	13.655219	-0.059778	4.816039
294.470345	8000.135511	13.660224	-0.059810	4.816049
294.565078	8000.123339	13.665229	-0.059828	4.816045
294.287672	8000.123627	13.670234	-0.059776	4.816047
294.658795	8000.142135	13.675239	-0.059845	4.816050
294.465024	8000.094788	13.680243	-0.059809	4.816038
294.306731	8000.098313	13.685248	-0.059780	4.816040
294.404638	8000.107572	13.690253	-0.059798	4.816042
294.486763	8000.119749	13.695258	-0.059813	4.816045
294.542040	8000.137849	13.700263	-0.059823	4.816050
294.325474	8000.091156	13.705267	-0.059783	4.816037
294.391020	8000.109443	13.710272	-0.059795	4.816042
294.419041	8000.130253	13.715277	-0.059800	4.816048
294.339297	8000.109561	13.720282	-0.059785	4.816043
294.483703	8000.134628	13.725287	-0.059812	4.816049
294.440682	8000.093231	13.730291	-0.059804	4.816037
294.223675	8000.060423	13.735296	-0.059764	4.816029
294.199883	8000.086701	13.740301	-0.059759	4.816037
294.187535	8000.084334	13.745306	-0.059757	4.816036
294.317439	8000.120891	13.750311	-0.059781	4.816046
294.345464	8000.110711	13.755315	-0.059786	4.816043
294.492718	8000.108044	13.760320	-0.059814	4.816041
294.424934	8000.105737	13.765325	-0.059801	4.816041
294.143270	8000.087781	13.770330	-0.059748	4.816037
294.451868	8000.125454	13.775335	-0.059806	4.816047
294.445636	8000.112512	13.780339	-0.059805	4.816043
294.413251	8000.108712	13.785344	-0.059799	4.816042
294.558199	8000.113484	13.790349	-0.059826	4.816043
294.433505	8000.098386	13.795354	-0.059802	4.816039
294.640420	8000.145964	13.800359	-0.059841	4.816052
294.481970	8000.089642	13.805363	-0.059811	4.816036
294.443425	8000.116720	13.810368	-0.059804	4.816044
294.487045	8000.134608	13.815373	-0.059812	4.816049
294.537169	8000.105594	13.820378	-0.059821	4.816040
294.597404	8000.136609	13.825383	-0.059833	4.816049
294.350162	8000.096837	13.830387	-0.059786	4.816039
294.383801	8000.114543	13.835392	-0.059793	4.816044
294.520692	8000.138404	13.840397	-0.059818	4.816050
294.543358	8000.087518	13.845402	-0.059822	4.816035
294.633241	8000.128690	13.850407	-0.059839	4.816047
294.449705	8000.113588	13.855411	-0.059805	4.816043
294.606359	8000.142084	13.860416	-0.059834	4.816051
294.712619	8000.137602	13.865421	-0.059854	4.816049
294.412819	8000.084050	13.870426	-0.059798	4.816035
294.358515	8000.100155	13.875431	-0.059788	4.816040
294.614317	8000.080229	13.880435	-0.059835	4.816033
294.481707	8000.073536	13.885440	-0.059810	4.816031
294.500650	8000.105935	13.890445	-0.059814	4.816041
294.511755	8000.086898	13.895450	-0.059816	4.816035
294.521020	8000.129807	13.900455	-0.059818	4.816048
294.249400	8000.101347	13.905459	-0.059767	4.816041
294.319736	8000.113310	13.910464	-0.059780	4.816044
294.662417	8000.121682	13.915469	-0.059844	4.816045
294.334381	8000.103950	13.920474	-0.059783	4.816041
294.323661	8000.093064	13.925479	-0.059781	4.816038
294.423401	8000.094875	13.930483	-0.059799	4.816038
294.427213	8000.093872	13.935488	-0.059800	4.816038
294.574545	8000.098687	13.940493	-0.059827	4.816038
294.302660	8000.093732	13.945498	-0.059777	4.816038
294.340172	8000.135019	13.950503	-0.059784	4.816050
294.282197	8000.107243	13.955507	-0.059773	4.816042
294.230303	8000.123392	13.960512	-0.059763	4.816047
294.303098	8000.128987	13.965517	-0.059777	4.816049
294.356059	8000.090407	13.970522	-0.059786	4.816037
294.409936	8000.134130	13.975527	-0.059796	4.816049
294.377855	8000.081178	13.980531	-0.059790	4.816034
294.379245	8000.068375	13.985536	-0.059790	4.816030
294.552247	8000.112129	13.990541	-0.059823	4.816042
294.362020	8000.115072	13.995546	-0.059787	4.816044
294.409558	8000.113796	14.000551	-0.059796	4.816044
294.415184	8000.073286	14.005555	-0.059797	4.816032
294.517391	8000.096515	14.010560	-0.059816	4.816038
294.652205	8000.137437	14.015565	-0.059841	4.816049
294.587632	8000.100991	14.020570	-0.059829	4.816039
294.484012	8000.120473	14.025575	-0.059810	4.816045
294.718058	8000.103357	14.030579	-0.059853	4.816039
294.654077	8000.092570	14.035584	-0.059841	4.816036
294.541516	8000.136467	14.040589	-0.059820	4.816049
294.257471	8000.072516	14.045594	-0.059767	4.816032
294.557395	8000.088659	14.050599	-0.059823	4.816035
294.547379	8000.093815	14.055603	-0.059821	4.816037
294.409208	8000.081677	14.060608	-0.059795	4.816034
294.594039	8000.061528	14.065613	-0.059830	4.816027
294.295919	8000.059301	14.070618	-0.059774	4.816028
294.348989	8000.079499	14.075623	-0.059784	4.816034
294.410673	8000.070999	14.080627	-0.059795	4.816031
294.345131	8000.101861	14.085632	-0.059783	4.816040
294.477471	8000.130982	14.090637	-0.059808	4.816048
294.413654	8000.103099	14.095642	-0.059796	4.816040
294.588957	8000.118042	14.100647	-0.059828	4.816044
294.668933	8000.100258	14.105651	-0.059843	4.816038
294.595989	8000.090377	14.110656	-0.059830	4.816036
294.697945	8000.140318	14.115661	-0.059849	4.816050
294.474295	8000.104181	14.120666	-0.059807	4.816040
294.497507	8000.114217	14.125671	-0.059811	4.816043
294.528433	8000.083785	14.130675	-0.059817	4.816034
294.468747	8000.102998	14.135680	-0.059806	4.816040
294.394074	8000.123007	14.140685	-0.059792	4.816046
294.455257	8000.093126	14.145690	-0.059803	4.816037
294.419803	8000.105300	14.150695	-0.059797	4.816041
294.444385	8000.083301	14.155699	-0.059801	4.816035
294.365184	8000.042315	14.160704	-0.059786	4.816023
294.538507	8000.106379	14.165709	-0.059818	4.816041
294.611077	8000.078843	14.170714	-0.059832	4.816032
294.551486	8000.078822	14.175719	-0.059821	4.816033
294.725793	8000.078785	14.180723	-0.059853	4.816032
294.810803	8000.037583	14.185728	-0.059869	4.816019
294.772876	8000.082840	14.190733	-0.059862	4.816033
294.497937	8000.007299	14.195738	-0.059811	4.816012
294.784310	8000.077696	14.200743	-0.059864	4.816031
294.694985	8000.084614	14.205747	-0.059847	4.816034
294.516195	8000.053569	14.210752	-0.059814	4.816025
294.545429	8000.109666	14.215757	-0.059819	4.816042
294.526258	8000.072979	14.220762	-0.059816	4.816031
294.503230	8000.105683	14.225767	-0.059811	4.816041
294.507379	8000.090793	14.230771	-0.059812	4.816036
294.419061	8000.102004	14.235776	-0.059796	4.816040
294.590176	8000.123282	14.240781	-0.059827	4.816045
294.450452	8000.053409	14.245786	-0.059801	4.816026
294.440522	8000.086352	14.250791	-0.059799	4.816035
294.468360	8000.107159	14.255795	-0.059805	4.816041
294.362701	7999.152032	14.260800	-0.059784	4.815763

294.442471	7995.989721	14.265805	-0.059797	4.814838
294.472212	7990.571288	14.270810	-0.059799	4.813255
294.429353	7983.904216	14.275815	-0.059787	4.811306
294.395234	7976.618948	14.280819	-0.059775	4.809175
294.382065	7969.006641	14.285824	-0.059768	4.806947
294.439063	7961.219979	14.290829	-0.059773	4.804667
294.206297	7953.413939	14.295834	-0.059725	4.802382
294.209588	7945.387767	14.300839	-0.059720	4.800030
294.221254	7937.468938	14.305843	-0.059717	4.797708
294.027236	7929.400529	14.310848	-0.059676	4.795342
293.965793	7921.456392	14.315853	-0.059659	4.793011
293.933687	7913.348674	14.320858	-0.059648	4.790630
294.097529	7905.440425	14.325863	-0.059673	4.788306
294.116365	7897.418997	14.330867	-0.059671	4.785949
293.923608	7889.439636	14.335872	-0.059630	4.783603
294.035853	7881.429689	14.340877	-0.059646	4.781246
293.848826	7873.407471	14.345882	-0.059606	4.778885
293.856607	7865.468511	14.350887	-0.059602	4.776547
293.879500	7857.410787	14.355891	-0.059601	4.774173
293.633460	7849.370105	14.360896	-0.059550	4.771804
293.713242	7841.361470	14.365901	-0.059560	4.769441
293.517123	7833.414231	14.370906	-0.059518	4.767097
293.525664	7825.362831	14.375911	-0.059514	4.764720
293.429224	7817.439756	14.380915	-0.059491	4.762380
293.438412	7809.338282	14.385920	-0.059487	4.759986
293.496936	7801.474840	14.390925	-0.059493	4.757661
293.289022	7793.372215	14.395930	-0.059449	4.755264
293.312400	7785.363235	14.400935	-0.059448	4.752894
293.338024	7777.370928	14.405939	-0.059448	4.750527
293.115666	7769.338399	14.410944	-0.059401	4.748148
293.174246	7761.376645	14.415949	-0.059407	4.745788
293.219673	7753.355531	14.420954	-0.059410	4.743409
293.208851	7745.341966	14.425959	-0.059403	4.741031
293.002423	7737.383749	14.430963	-0.059359	4.738669
292.925310	7729.335458	14.435968	-0.059339	4.736279
293.156979	7721.367262	14.440973	-0.059377	4.733911
292.987211	7713.309242	14.445978	-0.059340	4.731515
292.918357	7705.341479	14.450983	-0.059322	4.729145
292.986469	7697.336227	14.455987	-0.059330	4.726763
292.841185	7689.288705	14.460992	-0.059297	4.724367
292.654167	7681.353852	14.465997	-0.059257	4.722004
292.735298	7673.318986	14.471002	-0.059267	4.719608
292.740291	7665.375329	14.476007	-0.059263	4.717239
292.523720	7657.350848	14.481011	-0.059217	4.714846
292.436132	7649.301458	14.486016	-0.059195	4.712443
292.534217	7641.295590	14.491021	-0.059208	4.710052
292.521275	7633.356445	14.496026	-0.059201	4.707679
292.329481	7625.296510	14.501031	-0.059160	4.705270
292.484818	7617.362811	14.506035	-0.059184	4.702896
292.412098	7609.294472	14.511040	-0.059165	4.700482
292.325277	7601.355278	14.516045	-0.059143	4.698105
292.605055	7593.302327	14.521050	-0.059190	4.695691
292.467613	7585.319812	14.526055	-0.059159	4.693299
292.308570	7577.303792	14.531059	-0.059124	4.690895
292.296137	7569.294118	14.536064	-0.059117	4.688492
292.327216	7561.293049	14.541069	-0.059117	4.686090
291.917906	7553.267927	14.546074	-0.059036	4.683680
292.056320	7545.303960	14.551079	-0.059056	4.681287
292.159239	7537.361423	14.556083	-0.059070	4.678898
291.964364	7529.335834	14.561088	-0.059029	4.676484
292.093910	7521.270959	14.566093	-0.059048	4.674057
291.765038	7513.153443	14.571098	-0.058981	4.671613
291.697065	7505.203508	14.576103	-0.058963	4.669218
291.707339	7497.233303	14.581107	-0.058960	4.666815
291.634340	7489.192221	14.586112	-0.058941	4.664390
291.861272	7481.274929	14.591117	-0.058978	4.662000
291.729612	7473.220143	14.596122	-0.058948	4.659568
291.480857	7465.288873	14.601127	-0.058897	4.657173
291.648542	7457.225471	14.606131	-0.058923	4.654736
291.529869	7449.247445	14.611136	-0.058895	4.652323
291.476463	7441.245025	14.616141	-0.058880	4.649902
291.254925	7433.239883	14.621146	-0.058834	4.647479
291.278538	7425.193658	14.626151	-0.058833	4.645042
291.039091	7417.245369	14.631155	-0.058783	4.642634
291.079088	7409.226182	14.636160	-0.058785	4.640202
291.182981	7401.282414	14.641165	-0.058799	4.637793
291.109681	7393.200230	14.646170	-0.058780	4.635340
291.028059	7385.212783	14.651175	-0.058760	4.632914
291.141581	7377.167479	14.656179	-0.058776	4.630470
291.084313	7369.190595	14.661184	-0.058760	4.628045
290.812745	7361.175291	14.666189	-0.058704	4.625607
290.963353	7353.215599	14.671194	-0.058727	4.623185
290.974839	7345.213591	14.676199	-0.058723	4.620748
290.725733	7337.248068	14.681203	-0.058672	4.618322
290.575545	7329.179496	14.686208	-0.058639	4.615863
290.613310	7321.184169	14.691213	-0.058640	4.613424
290.566564	7313.142819	14.696218	-0.058626	4.610971
290.424943	7305.156778	14.701223	-0.058595	4.608533
290.426130	7297.185392	14.706227	-0.058590	4.606098
290.395183	7289.150798	14.711232	-0.058579	4.603642
290.288922	7281.197019	14.716237	-0.058554	4.601210
290.101202	7273.200528	14.721242	-0.058513	4.598764
290.271964	7265.163602	14.726247	-0.058540	4.596304
290.194009	7257.183899	14.731251	-0.058520	4.593860
290.044388	7249.088302	14.736256	-0.058487	4.591379
290.095366	7241.157925	14.741261	-0.058491	4.588948
289.922393	7233.109763	14.746266	-0.058454	4.586479
289.998670	7225.159386	14.751271	-0.058463	4.584039
290.114384	7217.138990	14.756275	-0.058479	4.581576
290.239719	7209.132003	14.761280	-0.058497	4.579116
290.102274	7201.165156	14.766285	-0.058466	4.576666
290.049072	7193.156846	14.771290	-0.058451	4.574203
289.758953	7185.135027	14.776295	-0.058392	4.571734
289.880293	7177.139184	14.781299	-0.058409	4.569272
289.596773	7169.118065	14.786304	-0.058351	4.566801
289.829698	7161.120478	14.791309	-0.058389	4.564336
289.613678	7153.155567	14.796314	-0.058344	4.561879
289.542307	7145.113737	14.801319	-0.058325	4.559397
289.610335	7137.192174	14.806323	-0.058333	4.556952
289.583035	7129.133690	14.811328	-0.058322	4.554462
289.545447	7121.140253	14.816333	-0.058310	4.551991
289.300142	7113.084279	14.821338	-0.058259	4.549500
289.226401	7105.128020	14.826343	-0.058240	4.547038
289.394403	7097.086462	14.831347	-0.058266	4.544548
289.372754	7089.149770	14.836352	-0.058257	4.542090
289.252893	7081.107036	14.841357	-0.058229	4.539597
289.216199	7073.165028	14.846362	-0.058217	4.537134
289.154675	7065.101730	14.851367	-0.058200	4.534632
289.132449	7057.113101	14.856371	-0.058191	4.532152
289.122937	7049.032337	14.861376	-0.058184	4.529642
289.023890	7041.165415	14.866381	-0.058160	4.527196
288.970581	7033.082733	14.871386	-0.058145	4.524683
288.847601	7025.167470	14.876391	-0.058117	4.522220
288.872798	7017.125380	14.881395	-0.058116	4.519716
288.739365	7009.127775	14.886400	-0.058086	4.517225
288.761113	7001.127674	14.891405	-0.058085	4.514732
288.848654	6993.005456	14.896410	-0.058096	4.512199
288.877152	6984.993198	14.901415	-0.058096	4.509700
288.724997	6977.082585	14.906419	-0.058063	4.507230
288.708147	6969.017552	14.911424	-0.058054	4.504711
288.870103	6961.116553	14.916429	-0.058079	4.502242
288.708493	6953.070497	14.921434	-0.058044	4.499725
288.549083	6945.106808	14.926439	-0.058009	4.497233
288.651622	6937.070798	14.931443	-0.058023	4.494718
288.403952	6929.061967	14.936448	-0.057971	4.492209
288.386191	6921.054849	14.941453	-0.057963	4.489699
288.281574	6913.072854	14.946458	-0.057938	4.487196
288.445548	6905.014482	14.951463	-0.057963	4.484668
288.149472	6897.107783	14.956467	-0.057903	4.482185
288.077082	6889.042620	14.961472	-0.057884	4.479652
288.066719	6881.107614	14.966477	-0.057877	4.477158
288.114567	6873.053423	14.971482	-0.057881	4.474625
288.126346	6865.019998	14.976487	-0.057877	4.472098
288.189668	6857.028290	14.981491	-0.057884	4.469582
288.059808	6849.005327	14.986496	-0.057854	4.467055
288.167302	6841.028140	14.991501	-0.057869	4.464541
288.101399	6833.048290	14.996506	-0.057852	4.462024
288.149573	6825.043093	15.001511	-0.057855	4.459498
288.022329	6817.088782	15.006515	-0.057827	4.456987
287.986090	6809.001673	15.011520	-0.057814	4.454432
287.833366	6801.029140	15.016525	-0.057781	4.451912
287.714069	6792.989756	15.021530	-0.057753	4.449369
287.744904	6785.013469	15.026535	-0.057754	4.446845
287.622644	6777.019833	15.031539	-0.057726	4.444314
287.681552	6769.016837	15.036544	-0.057731	4.441778
287.799429	6761.052148	15.041549	-0.057748	4.439254
287.744020	6753.060613	15.046554	-0.057733	4.436720
287.689212	6745.024491	15.051559	-0.057717	4.434169
287.310136	6736.999087	15.056563	-0.057641	4.431619
287.190070	6728.962367	15.061568	-0.057614	4.429066
287.502231	6720.983614	15.066573	-0.057667	4.426531
287.420655	6712.937986	15.071578	-0.057646	4.423971
287.399705	6704.981561	15.076583	-0.057637	4.421439
287.273533	6696.975277	15.081587	-0.057608	4.418889
287.312076	6688.944950	15.086592	-0.057610	4.416330
287.126958	6680.990931	15.091597	-0.057570	4.413794
287.142775	6672.956526	15.096602	-0.057568	4.411231
286.921145	6664.947812	15.101607	-0.057521	4.408674
286.848074	6656.957310	15.106611	-0.057503	4.406121
287.065940	6648.950568	15.111616	-0.057538	4.403564
286.963571	6641.000053	15.116621	-0.057514	4.401021
286.901984	6633.014539	15.121626	-0.057497	4.398466
286.946706	6625.007688	15.126631	-0.057500	4.395903
286.881448	6616.977977	15.131635	-0.057483	4.393331
286.750183	6608.915089	15.136640	-0.057453	4.390747
286.806227	6600.959134	15.141645	-0.057458	4.388196
286.798845	6592.966018	15.146650	-0.057451	4.385631
286.661601	6585.024430	15.151655	-0.057421	4.383080
286.556349	6576.991783	15.156659	-0.057396	4.380500
286.393604	6568.993043	15.161664	-0.057360	4.377928
286.445058	6561.009035	15.166669	-0.057364	4.375360
286.476388	6552.966034	15.171674	-0.057365	4.372772
286.488357	6544.915527	15.176679	-0.057362	4.370180
286.401707	6537.002303	15.181683	-0.057341	4.367630
286.358651	6528.924515	15.186688	-0.057327	4.365025
286.061711	6521.069952	15.191693	-0.057267	4.362490
285.870312	6512.987060	15.196698	-0.057226	4.359880
285.955819	6504.996799	15.201703	-0.057237	4.357300
285.833062	6497.040210	15.206707	-0.057208	4.354728
285.781652	6488.871794	15.211712	-0.057194	4.352086
285.860262	6480.883407	15.216717	-0.057203	4.349502
285.944820	6472.924697	15.221722	-0.057213	4.346926
285.748610	6464.928881	15.226727	-0.057172	4.344335
285.780503	6457.001848	15.231731	-0.057172	4.341766
285.628649	6448.945499	15.236736	-0.057139	4.339152
285.631567	6440.973711	15.241741	-0.057134	4.336565
285.544546	6432.934479	15.246746	-0.057113	4.333954
285.532301	6424.915911	15.251751	-0.057105	4.331349
285.580925	6416.976779	15.256755	-0.057109	4.328769
285.508812	6408.929727	15.261760	-0.057090	4.326150
285.698586	6400.955000	15.266765	-0.057120	4.323556
285.382772	6392.984129	15.271770	-0.057056	4.320958
285.322888	6384.968698	15.276775	-0.057040	4.318345
285.338464	6376.988117	15.281779	-0.057037	4.315743
285.168997	6368.873826	15.286784	-0.057001	4.313095
285.063972	6360.903719	15.291789	-0.056976	4.310492
285.016664	6352.910453	15.296794	-0.056962	4.307880
284.989946	6344.910147	15.301799	-0.056951	4.305265
285.075565	6336.962778	15.306803	-0.056962	4.302666
285.029743	6328.919207	15.311808	-0.056948	4.300033
285.049426	6320.962965	15.316813	-0.056947	4.297428
285.094832	6312.917613	15.321818	-0.056950	4.294792
284.837875	6304.934653	15.326823	-0.056897	4.292173
284.988599	6296.911944	15.331827	-0.056920	4.289542
284.805120	6288.916247	15.336832	-0.056880	4.286916
284.584737	6280.940662	15.341837	-0.056834	4.284294
284.414453	6272.932772	15.346842	-0.056797	4.281661
284.654317	6264.920921	15.351847	-0.056836	4.279028
284.635535	6256.943925	15.356851	-0.056828	4.276402
284.476608	6248.887138	15.361856	-0.056793	4.273748
284.533231	6240.878402	15.366861	-0.056798	4.271110
284.448804	6232.891371	15.371866	-0.056777	4.268475
284.227628	6224.842745	15.376871	-0.056731	4.265818
284.464562	6216.889731	15.381875	-0.056770	4.263195
284.358943	6208.909642	15.386880	-0.056745	4.260558
284.207354	6200.927229	15.391885	-0.056711	4.257918
284.080590	6192.910500	15.396890	-0.056682	4.255266
284.216206	6184.862740	15.401895	-0.056702	4.252604
284.257463	6176.917649	15.406899	-0.056705	4.249973
284.040739	6168.899535	15.411904	-0.056659	4.247315
284.261254	6160.884273	15.416909	-0.056695	4.244659
283.961037	6152.970739	15.421914	-0.056634	4.242031
283.787065	6144.938480	15.426919	-0.056596	4.239363
283.940169	6136.976653	15.431923	-0.056619	4.236719
283.853861	6128.898624	15.436928	-0.056598	4.234034
283.965887	6120.869068	15.441933	-0.056614	4.231364
283.766530	6112.903862	15.446938	-0.056571	4.228711
283.552294	6104.863565	15.451943	-0.056526	4.226032
283.687183	6096.933792	15.456947	-0.056546	4.223390
283.417698	6088.907188	15.461952	-0.056490	4.220711
283.459008	6080.969494	15.466957	-0.056493	4.218063
283.694839	6072.942357	15.471962	-0.056532	4.215386
283.618750	6064.886320	15.476967	-0.056512	4.212693
283.761892	6056.911217	15.481971	-0.056533	4.210029
283.556239	6048.888870	15.486976	-0.056490	4.207343
283.434951	6040.916790	15.491981	-0.056462	4.204674
283.276551	6032.956529	15.496986	-0.056427	4.202006
283.290064	6024.951534	15.501991	-0.056425	4.199323
283.472462	6016.966097	15.506995	-0.056453	4.196647
282.985384	6008.876776	15.512000	-0.056357	4.193927
283.017975	6000.817896	15.517005	-0.056358	4.191222
283.231843	5992.853370	15.522010	-0.056393	4.188548
282.911121	5984.854731	15.527015	-0.056328	4.185855
282.920633	5976.915082	15.532019	-0.056324	4.183184
282.800343	5968.867777	15.537024	-0.056297	4.180473
282.859043	5960.909031	15.542029	-0.056302	4.177793
282.618867	5952.862109	15.547034	-0.056252	4.175077
282.649174	5944.886822	15.552039	-0.056253	4.172387
282.591535	5936.918578	15.557043	-0.056237	4.169697
282.410575	5928.884655	15.562048	-0.056198	4.166982
282.597592	5920.889314	15.567053	-0.056227	4.164281
282.554185	5912.941706	15.572058	-0.056214	4.161593
282.352825	5904.890110	15.577063	-0.056171	4.158866
282.427773	5896.900160	15.582067	-0.056180	4.156161
282.343388	5888.841495	15.587072	-0.056159	4.153429
282.611676	5880.867465	15.592077	-0.056204	4.150729
282.278756	5872.888452	15.597082	-0.056136	4.148017
282.299345	5864.860522	15.602087	-0.056135	4.145292
282.270589	5856.925903	15.607091	-0.056124	4.142596
281.853038	5848.905163	15.612096	-0.056041	4.139864
281.843573	5840.938192	15.617101	-0.056034	4.137153
281.883507	5832.899563	15.622106	-0.056036	4.134417
281.789920	5824.842508	15.627111	-0.056014	4.131672
281.858235	5816.884051	15.632115	-0.056021	4.128959
281.887362	5808.841606	15.637120	-0.056021	4.126216
281.931190	5800.850614	15.642125	-0.056024	4.123489
281.721892	5792.873933	15.647130	-0.055980	4.120762
281.820528	5784.905272	15.652135	-0.055993	4.118040
281.880689	5776.895785	15.657139	-0.055999	4.115301
281.674037	5768.821955	15.662144	-0.055955	4.112535
281.465885	5760.824786	15.667149	-0.055911	4.109794
281.479259	5752.889583	15.672154	-0.055909	4.107075
281.315907	5744.869684	15.677159	-0.055873	4.104322
281.368194	5736.931828	15.682163	-0.055877	4.101599
281.415557	5728.873991	15.687168	-0.055881	4.098833
281.386604	5720.876210	15.692173	-0.055870	4.096084
281.305024	5712.876722	15.697178	-0.055850	4.093332
281.304669	5704.866883	15.702183	-0.055845	4.090576
281.355296	5696.909457	15.707187	-0.055849	4.087837
281.095150	5688.909450	15.712192	-0.055795	4.085077
281.075946	5680.955491	15.717197	-0.055786	4.082334
281.164653	5672.874277	15.722202	-0.055797	4.079547
281.227809	5664.915253	15.727207	-0.055804	4.076800
281.094261	5656.897885	15.732211	-0.055774	4.074029
281.069587	5648.882670	15.737216	-0.055764	4.071257
280.973954	5640.916322	15.742221	-0.055741	4.068500
280.909070	5632.914538	15.747226	-0.055724	4.065729
280.822352	5624.923618	15.752231	-0.055702	4.062959
280.944056	5616.920853	15.757235	-0.055720	4.060187
280.891320	5608.944016	15.762240	-0.055704	4.057419
280.695736	5600.948751	15.767245	-0.055663	4.054640
280.683673	5592.938134	15.772250	-0.055655	4.051857
280.641395	5584.877704	15.777255	-0.055642	4.049055
280.554143	5576.911747	15.782259	-0.055621	4.046283
280.299684	5568.918729	15.787264	-0.055568	4.043496
280.355947	5560.922962	15.792269	-0.055573	4.040712
280.327603	5552.953218	15.797274	-0.055563	4.037933
280.250035	5544.930195	15.802279	-0.055543	4.035134
280.183898	5536.852400	15.807283	-0.055525	4.032313
280.156360	5528.817083	15.812288	-0.055515	4.029506
280.115907	5520.886141	15.817293	-0.055502	4.026733
280.144682	5512.847110	15.822298	-0.055502	4.023921
280.051683	5504.899137	15.827303	-0.055480	4.021137
279.982632	5496.912920	15.832307	-0.055462	4.018339
279.952524	5488.893231	15.837312	-0.055451	4.015527
279.733808	5480.905142	15.842317	-0.055405	4.012722
280.000557	5472.854498	15.847322	-0.055449	4.009900
279.537367	5464.908836	15.852327	-0.055358	4.007101
279.730535	5456.915257	15.857331	-0.055388	4.004294
279.618778	5448.899842	15.862336	-0.055362	4.001473
279.513801	5440.893382	15.867341	-0.055338	3.998653
279.697239	5432.887765	15.872346	-0.055366	3.995836
279.601596	5424.856813	15.877351	-0.055343	3.993003
279.555079	5416.877176	15.882355	-0.055329	3.990187
279.580158	5408.876102	15.887360	-0.055329	3.987363
279.550933	5400.873434	15.892365	-0.055318	3.984536
279.651525	5392.944720	15.897370	-0.055332	3.981734
279.368667	5384.921727	15.902375	-0.055274	3.978891
279.426736	5376.903950	15.907379	-0.055279	3.976054
279.598229	5368.890182	15.912384	-0.055306	3.973217
279.379667	5360.880740	15.917389	-0.055260	3.970374
279.386991	5352.929980	15.922394	-0.055256	3.967553
279.231992	5344.888724	15.927399	-0.055222	3.964696
279.195376	5336.976917	15.932403	-0.055210	3.961884
279.149304	5328.914955	15.937408	-0.055196	3.959017
279.127918	5320.970841	15.942413	-0.055187	3.956190
278.905617	5312.936769	15.947418	-0.055140	3.953326
278.720282	5304.887593	15.952423	-0.055100	3.950454
278.819865	5296.940138	15.957427	-0.055114	3.947622
278.686082	5288.915097	15.962432	-0.055083	3.944756
278.760478	5280.970692	15.967437	-0.055092	3.941920
278.828753	5272.971145	15.972442	-0.055100	3.939063
278.624048	5264.969697	15.977447	-0.055056	3.936198
278.651240	5256.978555	15.982451	-0.055056	3.933338
278.580497	5248.914362	15.987456	-0.055038	3.930449
278.784745	5240.981067	15.992461	-0.055070	3.927609
278.677424	5232.940900	15.997466	-0.055045	3.924723
278.483205	5225.004909	16.002471	-0.055004	3.921871
278.368676	5216.965687	16.007475	-0.054977	3.918982
278.159120	5208.995365	16.012480	-0.054933	3.916113
278.157201	5200.960708	16.017485	-0.054927	3.913222
278.122187	5192.957935	16.022490	-0.054915	3.910341
278.126605	5184.939166	16.027495	-0.054911	3.907452
278.072714	5176.963050	16.032499	-0.054896	3.904575
277.766580	5169.025581	16.037504	-0.054833	3.901706
277.833111	5160.992926	16.042509	-0.054841	3.898807
277.883910	5152.971351	16.047514	-0.054845	3.895909
277.817236	5144.927257	16.052519	-0.054827	3.892999
277.792058	5136.936226	16.057523	-0.054817	3.890107
277.687811	5128.990591	16.062528	-0.054792	3.887228
277.638552	5120.955891	16.067533	-0.054778	3.884315
277.632455	5112.999850	16.072538	-0.054772	3.881429
277.543903	5104.993874	16.077543	-0.054750	3.878522
277.625026	5096.998756	16.082547	-0.054760	3.875619
277.580670	5088.775844	16.087552	-0.054746	3.872629
277.440190	5080.778021	16.092557	-0.054715	3.869717
277.307756	5072.876723	16.097562	-0.054685	3.866838
277.217028	5064.901194	16.102567	-0.054663	3.863930
277.165150	5056.956164	16.107571	-0.054648	3.861033
277.265012	5048.943953	16.112576	-0.054661	3.858111
277.259834	5040.957128	16.117581	-0.054655	3.855194
277.033947	5032.966976	16.122586	-0.054608	3.852270
276.866481	5024.947390	16.127591	-0.054571	3.849334
277.081958	5016.942072	16.132595	-0.054606	3.846408
276.882592	5008.972320	16.137600	-0.054564	3.843485
276.735076	5001.053549	16.142605	-0.054531	3.840579
276.950608	4993.047631	16.147610	-0.054566	3.837647
277.040105	4985.002875	16.152615	-0.054577	3.834695
277.023557	4977.016046	16.157619	-0.054569	3.831761
276.744936	4968.972736	16.162624	-0.054512	3.828798
276.635504	4960.989066	16.167629	-0.054486	3.825858
276.482887	4953.068252	16.172634	-0.054452	3.822938
276.339136	4945.031969	16.177639	-0.054420	3.819973
276.317669	4937.066151	16.182643	-0.054411	3.817034
276.220609	4929.058354	16.187648	-0.054388	3.814077
276.356673	4921.009743	16.192653	-0.054408	3.811106
276.221565	4913.026753	16.197658	-0.054377	3.808152
276.082459	4905.003016	16.202663	-0.054346	3.805181
276.319787	4897.049919	16.207667	-0.054385	3.802241
276.158108	4889.045910	16.212672	-0.054350	3.799272
276.339187	4881.078025	16.217677	-0.054378	3.796321
276.296351	4873.056965	16.222682	-0.054365	3.793343
276.164350	4865.002059	16.227687	-0.054335	3.790349
276.504543	4857.023333	16.232691	-0.054393	3.787390
276.142338	4849.020644	16.237696	-0.054321	3.784405
276.073170	4841.097696	16.242701	-0.054303	3.781454
276.085413	4833.066434	16.247706	-0.054300	3.778462
275.902383	4825.062323	16.252711	-0.054260	3.775473
275.908720	4817.086818	16.257715	-0.054256	3.772497
275.729256	4809.044310	16.262720	-0.054217	3.769489
275.703082	4801.068422	16.267725	-0.054207	3.766507
275.711163	4793.073451	16.272730	-0.054204	3.763517
275.427337	4785.087432	16.277735	-0.054145	3.760521
275.484087	4777.109798	16.282739	-0.054151	3.757533
275.368128	4769.059920	16.287744	-0.054124	3.754512
275.405934	4761.067923	16.292749	-0.054126	3.751513
275.429474	4753.057419	16.297754	-0.054125	3.748505
275.244082	4745.054518	16.302759	-0.054085	3.745493
275.358738	4737.074544	16.307763	-0.054101	3.742494
275.393554	4729.076005	16.312768	-0.054102	3.739483
275.302694	4721.130600	16.317773	-0.054080	3.736487
275.497632	4713.087813	16.322778	-0.054111	3.733459
275.250019	4705.062479	16.327783	-0.054060	3.730424
275.259656	4697.131834	16.332787	-0.054056	3.727429
275.087499	4689.075305	16.337792	-0.054019	3.724379
274.951693	4681.156803	16.342797	-0.053989	3.721380
275.018318	4673.149572	16.347802	-0.053996	3.718350
275.014531	4665.154944	16.352807	-0.053990	3.715321
275.068294	4657.094897	16.357811	-0.053994	3.712265
274.773181	4649.070238	16.362816	-0.053934	3.709212
274.863922	4641.058922	16.367821	-0.053946	3.706171
274.838202	4633.133013	16.372826	-0.053936	3.703157
274.933558	4625.113125	16.377831	-0.053948	3.700108
274.895705	4617.173127	16.382835	-0.053936	3.697083
274.734377	4609.128898	16.387840	-0.053901	3.694013
274.597320	4601.156129	16.392845	-0.053870	3.690969
274.748083	4593.181932	16.397850	-0.053893	3.687928
274.647831	4585.157916	16.402855	-0.053869	3.684860
274.636594	4577.240908	16.407859	-0.053862	3.681832
274.233495	4569.207707	16.412864	-0.053781	3.678748
274.329153	4561.206481	16.417869	-0.053794	3.675685
274.415041	4553.197064	16.422874	-0.053805	3.672617
274.244297	4545.163295	16.427879	-0.053767	3.669530
274.271873	4537.219920	16.432883	-0.053767	3.666481
274.337794	4529.211576	16.437888	-0.053774	3.663404
274.301382	4521.189180	16.442893	-0.053762	3.660318
274.294348	4513.238890	16.447898	-0.053756	3.657257
274.061181	4505.225397	16.452903	-0.053707	3.654163
273.948616	4497.223631	16.457907	-0.053681	3.651075
273.888573	4489.216253	16.462912	-0.053664	3.647983
274.050133	4481.181305	16.467917	-0.053689	3.644883
273.913464	4473.277502	16.472922	-0.053659	3.641824
273.817367	4465.241345	16.477927	-0.053635	3.638712
273.934872	4457.270855	16.482931	-0.053652	3.635628
273.850424	4449.200140	16.487936	-0.053631	3.632498
273.724694	4441.172245	16.492941	-0.053602	3.629380
273.570470	4433.216768	16.497946	-0.053568	3.626287
273.577239	4425.229730	16.502951	-0.053564	3.623184
273.404889	4417.273179	16.507955	-0.053527	3.620085
273.286743	4409.286891	16.512960	-0.053500	3.616972
273.244805	4401.286207	16.517965	-0.053487	3.613854
273.425493	4393.235289	16.522970	-0.053515	3.610720
273.213848	4385.270741	16.527975	-0.053470	3.607606
273.212996	4377.268007	16.532979	-0.053465	3.604479
273.146596	4369.332713	16.537984	-0.053447	3.601375
273.129963	4361.295510	16.542989	-0.053439	3.598230
273.260248	4353.318688	16.547994	-0.053458	3.595109
273.214242	4345.312696	16.552999	-0.053444	3.591970
273.148453	4337.315138	16.558003	-0.053427	3.588830
272.864306	4329.353718	16.563008	-0.053369	3.585696
272.934898	4321.373198	16.568013	-0.053377	3.582562
272.863052	4313.362264	16.573018	-0.053358	3.579409
272.509627	4305.403270	16.578023	-0.053287	3.576265
272.629474	4297.384807	16.583027	-0.053304	3.573109
272.572027	4289.331620	16.588032	-0.053288	3.569931
272.488321	4281.363431	16.593037	-0.053267	3.566783
272.582442	4273.352257	16.598042	-0.053279	3.563620
272.527677	4265.363757	16.603047	-0.053264	3.560460
272.490432	4257.422097	16.608051	-0.053252	3.557315
272.566867	4249.366499	16.613056	-0.053261	3.554126
272.426170	4241.288429	16.618061	-0.053229	3.550919
272.386885	4233.353352	16.623066	-0.053217	3.547768
272.191951	4225.337086	16.628071	-0.053175	3.544578
272.324742	4217.385462	16.633075	-0.053195	3.541421
272.232342	4209.363513	16.638080	-0.053172	3.538226
272.259322	4201.380700	16.643085	-0.053172	3.535047
272.246630	4193.400199	16.648090	-0.053164	3.531865
272.221415	4185.397339	16.653095	-0.053154	3.528671
272.298352	4177.400320	16.658099	-0.053163	3.525479
272.000559	4169.452785	16.663104	-0.053103	3.522293
271.714093	4161.450115	16.668109	-0.053044	3.519082
271.934043	4153.484339	16.673114	-0.053080	3.515899
271.679885	4145.465133	16.678119	-0.053027	3.512677
271.590175	4137.445561	16.683123	-0.053005	3.509456
271.593328	4129.444185	16.688128	-0.053001	3.506243
271.520886	4121.453600	16.693133	-0.052982	3.503029
271.669937	4113.459610	16.698138	-0.053004	3.499817
271.397366	4105.499105	16.703143	-0.052948	3.496603
271.691985	4097.472146	16.708147	-0.052998	3.493377
271.553140	4089.456569	16.713152	-0.052967	3.490139
271.541397	4081.504342	16.718157	-0.052959	3.486927
271.713602	4073.534359	16.723162	-0.052986	3.483711
271.440480	4065.543849	16.728167	-0.052930	3.480470
271.419667	4057.578215	16.733171	-0.052921	3.477244
271.286223	4049.576446	16.738176	-0.052891	3.473996
271.031404	4041.536366	16.743181	-0.052838	3.470726
270.835004	4033.572397	16.748186	-0.052796	3.467486
271.075458	4025.511671	16.753191	-0.052836	3.464217
271.274577	4017.546851	16.758195	-0.052868	3.460983
270.969993	4009.600935	16.763200	-0.052806	3.457738
270.600647	4001.595040	16.768205	-0.052732	3.454462
270.783706	3993.562886	16.773210	-0.052760	3.451191
270.608924	3985.567587	16.778215	-0.052723	3.447920
270.635256	3977.567690	16.783219	-0.052722	3.444651
270.629585	3969.632096	16.788224	-0.052716	3.441404
270.468499	3961.631156	16.793229	-0.052681	3.438121
270.576876	3953.633732	16.798234	-0.052696	3.434846
270.602472	3945.589739	16.803239	-0.052695	3.431546
270.558089	3937.621441	16.808243	-0.052682	3.428272
270.547847	3929.599567	16.813248	-0.052675	3.424974
270.381811	3921.658009	16.818253	-0.052638	3.421700
270.412391	3913.642193	16.823258	-0.052639	3.418399
270.303690	3905.659119	16.828263	-0.052613	3.415104
270.056381	3897.704236	16.833267	-0.052562	3.411812
270.036637	3889.657639	16.838272	-0.052553	3.408487
270.008498	3881.696568	16.843277	-0.052543	3.405194
270.056065	3873.730184	16.848282	-0.052546	3.401898
269.730243	3865.744398	16.853287	-0.052480	3.398578
269.843554	3857.751982	16.858291	-0.052496	3.395268
269.883274	3849.654668	16.863296	-0.052498	3.391907
269.776269	3841.673705	16.868301	-0.052473	3.388587
269.789609	3833.680817	16.873306	-0.052470	3.385263
269.646778	3825.733581	16.878311	-0.052438	3.381949
269.754575	3817.759706	16.883315	-0.052453	3.378629
269.724637	3809.766309	16.888320	-0.052442	3.375293
269.483604	3801.762010	16.893325	-0.052392	3.371942
269.710716	3793.771030	16.898330	-0.052429	3.368610
269.422024	3785.775597	16.903335	-0.052370	3.365254
269.465434	3777.844281	16.908339	-0.052373	3.361933
269.284880	3769.828942	16.913344	-0.052334	3.358566
269.431494	3761.812427	16.918349	-0.052356	3.355207
269.596483	3753.793392	16.923354	-0.052382	3.351844
269.278778	3745.808831	16.928359	-0.052317	3.348475
269.162997	3737.835144	16.933363	-0.052291	3.345114
269.196624	3729.854454	16.938368	-0.052292	3.341752
269.179204	3721.855115	16.943373	-0.052283	3.338377
269.163913	3713.891038	16.948378	-0.052275	3.335014
268.891247	3705.875353	16.953383	-0.052219	3.331616
269.008856	3697.867287	16.958387	-0.052236	3.328232
268.891113	3689.892948	16.963392	-0.052208	3.324850
268.833255	3681.927450	16.968397	-0.052192	3.321471
268.582757	3673.985456	16.973402	-0.052141	3.318091
268.688696	3665.928645	16.978407	-0.052155	3.314672
268.658616	3657.900846	16.983411	-0.052144	3.311257
268.593138	3649.904252	16.988416	-0.052127	3.307850
268.414943	3641.918550	16.993421	-0.052088	3.304440
268.536547	3633.981981	16.998426	-0.052106	3.301059
268.365698	3626.000474	17.003431	-0.052069	3.297644
268.458183	3618.000297	17.008435	-0.052081	3.294228
268.608216	3609.942737	17.013440	-0.052103	3.290786
268.330217	3602.005999	17.018445	-0.052046	3.287375
268.424524	3594.023997	17.023450	-0.052059	3.283956
268.207476	3586.046162	17.028455	-0.052013	3.280523
268.243526	3578.076586	17.033459	-0.052014	3.277100
268.045769	3570.058734	17.038464	-0.051972	3.273643
267.999804	3562.018380	17.043469	-0.051958	3.270179
268.000041	3554.086632	17.048474	-0.051953	3.266760
267.855475	3546.073622	17.053479	-0.051921	3.263296
267.742212	3538.084412	17.058483	-0.051895	3.259840
267.739597	3530.113877	17.063488	-0.051889	3.256393
267.684088	3522.091015	17.068493	-0.051873	3.252918
267.708416	3514.087469	17.073498	-0.051873	3.249450
267.845780	3506.101536	17.078503	-0.051893	3.245991
267.689596	3498.144502	17.083507	-0.051859	3.242529
267.573003	3490.185948	17.088512	-0.051832	3.239064
267.556335	3482.188773	17.093517	-0.051823	3.235583
267.493790	3474.139997	17.098522	-0.051806	3.232074
267.421284	3466.130249	17.103527	-0.051788	3.228577
267.360932	3458.158819	17.108531	-0.051771	3.225094
267.328503	3450.203435	17.113536	-0.051760	3.221615
267.251394	3442.206629	17.118541	-0.051740	3.218112
267.185224	3434.220400	17.123546	-0.051723	3.214611
267.176154	3426.185634	17.128551	-0.051716	3.211087
267.217187	3418.229630	17.133555	-0.051718	3.207595
266.984487	3410.262521	17.138560	-0.051670	3.204084
266.998110	3402.286067	17.143565	-0.051667	3.200575
266.893676	3394.326647	17.148570	-0.051642	3.197065
266.967372	3386.297646	17.153575	-0.051651	3.193527
266.956814	3378.276292	17.158579	-0.051643	3.189986
267.026264	3370.300043	17.163584	-0.051651	3.186463
266.878502	3362.294682	17.168589	-0.051618	3.182915
266.657772	3354.358104	17.173594	-0.051572	3.179390
266.646283	3346.378113	17.178599	-0.051565	3.175851
266.631599	3338.367970	17.183603	-0.051557	3.172295
266.422275	3330.376337	17.188608	-0.051512	3.168734
266.445520	3322.360253	17.193613	-0.051511	3.165168
266.539795	3314.424818	17.198618	-0.051524	3.161638
266.294062	3306.460997	17.203623	-0.051473	3.158076
266.180653	3298.453671	17.208627	-0.051446	3.154496
266.225404	3290.423437	17.213632	-0.051449	3.150909
266.295225	3282.408964	17.218637	-0.051457	3.147326
266.317762	3274.430467	17.223642	-0.051456	3.143753
266.151667	3266.468263	17.228647	-0.051420	3.140175
266.064289	3258.485999	17.233651	-0.051398	3.136587
265.999835	3250.503734	17.238656	-0.051381	3.132996
265.825364	3242.501909	17.243661	-0.051343	3.129387
265.980465	3234.515850	17.248666	-0.051367	3.125796
265.783395	3226.556223	17.253671	-0.051325	3.122197
265.659743	3218.608317	17.258675	-0.051297	3.118602
265.599489	3210.608861	17.263680	-0.051280	3.114983
265.810329	3202.543673	17.268685	-0.051314	3.111342
265.756815	3194.571854	17.273690	-0.051299	3.107727
265.541216	3186.591734	17.278695	-0.051254	3.104096
265.493188	3178.639424	17.283699	-0.051240	3.100482
265.385583	3170.657755	17.288704	-0.051214	3.096847
265.418554	3162.632413	17.293709	-0.051215	3.093195
265.392220	3154.664908	17.298714	-0.051205	3.089562
265.333458	3146.673124	17.303719	-0.051189	3.085912
265.289177	3138.705761	17.308723	-0.051175	3.082270
265.320943	3130.702674	17.313728	-0.051176	3.078610
265.144341	3122.741002	17.318733	-0.051138	3.074955
265.125763	3114.668135	17.323738	-0.051129	3.071253
265.018960	3106.681907	17.328743	-0.051104	3.067581
265.067673	3098.724822	17.333747	-0.051108	3.063926
265.152472	3090.719981	17.338752	-0.051118	3.060246
265.050145	3082.749876	17.343757	-0.051094	3.056569
265.132448	3074.784108	17.348762	-0.051104	3.052898
264.785956	3066.805505	17.353767	-0.051034	3.049197
264.754064	3058.838964	17.358771	-0.051023	3.045511
264.863788	3050.860818	17.363776	-0.051038	3.041822
265.003307	3042.865676	17.368781	-0.051059	3.038123
264.920732	3034.911141	17.373786	-0.051039	3.034427
264.723203	3026.880174	17.378791	-0.050997	3.030686
264.960312	3018.884711	17.383795	-0.051035	3.026977
264.669065	3010.930875	17.388800	-0.050976	3.023258
264.560795	3002.944580	17.393805	-0.050951	3.019528
264.582884	2994.989402	17.398810	-0.050949	3.015814
264.370358	2986.991711	17.403815	-0.050905	3.012064
264.192207	2979.008503	17.408819	-0.050866	3.008318
264.313640	2970.986042	17.413824	-0.050883	3.004563
264.263328	2963.042724	17.418829	-0.050869	3.000833
264.043463	2955.098553	17.423834	-0.050823	2.997089
264.011514	2947.058463	17.428839	-0.050812	2.993304
264.084372	2939.059246	17.433843	-0.050820	2.989540
263.838284	2931.107030	17.438848	-0.050769	2.985776
263.745978	2923.118325	17.443853	-0.050746	2.981999
263.838824	2915.141957	17.448858	-0.050758	2.978231
263.947024	2907.127880	17.453863	-0.050773	2.974442
263.870179	2899.137707	17.458867	-0.050754	2.970650
263.734280	2891.193643	17.463872	-0.050723	2.966872
263.759400	2883.180889	17.468877	-0.050723	2.963065
263.798038	2875.213034	17.473882	-0.050725	2.959275
263.495776	2867.262405	17.478887	-0.050663	2.955471
263.654829	2859.239996	17.483891	-0.050687	2.951651
263.387840	2851.271714	17.488896	-0.050632	2.947830
263.269754	2843.282874	17.493901	-0.050605	2.944002
263.249080	2835.329806	17.498906	-0.050596	2.940192
263.466346	2827.330129	17.503911	-0.050631	2.936366
263.347618	2819.345299	17.508915	-0.050604	2.932525
263.313386	2811.343666	17.513920	-0.050592	2.928675
263.403041	2803.335877	17.518925	-0.050604	2.924824
263.212078	2795.435128	17.523930	-0.050563	2.921004
263.110131	2787.453687	17.528935	-0.050539	2.917146
263.167139	2779.402256	17.533939	-0.050544	2.913256
263.069452	2771.371384	17.538944	-0.050521	2.909363
262.868524	2763.413476	17.543949	-0.050478	2.905495
262.903316	2755.474459	17.548954	-0.050479	2.901644
262.914727	2747.478568	17.553959	-0.050476	2.897758
262.936357	2739.497400	17.558963	-0.050475	2.893875
262.551892	2731.537188	17.563968	-0.050398	2.889975
262.714457	2723.551734	17.568973	-0.050423	2.886087
262.744662	2715.583317	17.573978	-0.050423	2.882194
262.378867	2707.633247	17.578983	-0.050350	2.878284
262.422656	2699.638460	17.583987	-0.050353	2.874369
262.300173	2691.633636	17.588992	-0.050325	2.870435
262.044691	2683.678183	17.593997	-0.050272	2.866512
262.021494	2675.690047	17.599002	-0.050263	2.862581
262.122264	2667.710420	17.604007	-0.050276	2.858655
262.159324	2659.729242	17.609011	-0.050278	2.854719
262.266048	2651.710178	17.614016	-0.050292	2.850763
262.168301	2643.741590	17.619021	-0.050269	2.846816
262.113199	2635.789378	17.624026	-0.050253	2.842873
261.734076	2627.852113	17.629031	-0.050178	2.838914
261.696305	2619.888774	17.634035	-0.050165	2.834955
261.863164	2611.814313	17.639040	-0.050191	2.830948
261.502172	2603.854311	17.644045	-0.050119	2.826962
261.590137	2595.895338	17.649050	-0.050130	2.822996
261.418338	2587.930876	17.654055	-0.050093	2.819007
261.428472	2579.940814	17.659059	-0.050089	2.815010
261.260885	2571.970573	17.664064	-0.050053	2.811007
261.341246	2563.968472	17.669069	-0.050062	2.806996
261.168028	2556.035400	17.674074	-0.050025	2.803000
261.183712	2548.016401	17.679079	-0.050023	2.798966
261.021709	2540.082639	17.684083	-0.049987	2.794958
261.074186	2532.060824	17.689088	-0.049992	2.790913
261.087599	2524.047095	17.694093	-0.049989	2.786864
261.083850	2516.093835	17.699098	-0.049983	2.782838
260.865425	2508.149868	17.704103	-0.049937	2.778799
260.762956	2500.197973	17.709107	-0.049913	2.774757
260.828099	2492.179940	17.714112	-0.049920	2.770685
260.718405	2484.196461	17.719117	-0.049894	2.766614
260.992442	2476.189226	17.724122	-0.049940	2.762548
260.744029	2468.257703	17.729127	-0.049888	2.758483
260.549447	2460.298155	17.734131	-0.049847	2.754401
260.475011	2452.226171	17.739136	-0.049828	2.750263
260.363353	2444.272327	17.744141	-0.049802	2.746177
260.513978	2436.300150	17.749146	-0.049824	2.742091
260.373849	2428.359458	17.754151	-0.049793	2.737998
260.140499	2420.435660	17.759155	-0.049745	2.733902
260.185651	2412.388172	17.764160	-0.049748	2.729752
260.000222	2404.448404	17.769165	-0.049708	2.725638
260.206380	2396.463452	17.774170	-0.049741	2.721518
260.080733	2388.494363	17.779175	-0.049712	2.717380
260.112023	2380.500187	17.784179	-0.049713	2.713232
260.152400	2372.506933	17.789184	-0.049715	2.709079
259.913706	2364.568200	17.794189	-0.049666	2.704931
259.992825	2356.606785	17.799194	-0.049675	2.700784
259.983261	2348.630539	17.804199	-0.049668	2.696617
260.026158	2340.628727	17.809203	-0.049671	2.692434
260.069908	2332.637435	17.814208	-0.049674	2.688250
259.811905	2324.699020	17.819213	-0.049620	2.684068
259.865038	2316.743942	17.824218	-0.049625	2.679890
259.726509	2308.787625	17.829223	-0.049594	2.675693
259.611029	2300.773036	17.834227	-0.049567	2.671460
259.606661	2292.802068	17.839232	-0.049561	2.667251
259.476877	2284.832351	17.844237	-0.049532	2.663028
259.306048	2276.890346	17.849242	-0.049495	2.658810
259.329831	2268.892680	17.854247	-0.049494	2.654568
259.457628	2260.885714	17.859251	-0.049512	2.650321
259.233836	2252.948482	17.864256	-0.049466	2.646081
259.172491	2244.983467	17.869261	-0.049449	2.641831
259.127205	2237.026417	17.874266	-0.049435	2.637579
259.024460	2229.056023	17.879271	-0.049411	2.633309
258.797254	2221.083332	17.884275	-0.049363	2.629023
258.965003	2213.076637	17.889280	-0.049389	2.624738
258.770616	2205.136244	17.894285	-0.049348	2.620457
258.747352	2197.189557	17.899290	-0.049338	2.616177
258.530420	2189.208381	17.904295	-0.049293	2.611859
258.392613	2181.240263	17.909299	-0.049262	2.607545
258.365354	2173.297356	17.914304	-0.049252	2.603246
258.222379	2165.308852	17.919309	-0.049220	2.598907
258.374609	2157.320038	17.924314	-0.049243	2.594581
258.407796	2149.120640	17.929319	-0.049244	2.590124
258.285866	2141.212389	17.934323	-0.049216	2.585809
258.425175	2133.262178	17.939328	-0.049236	2.581480
258.331131	2125.328165	17.944333	-0.049214	2.577138
258.226629	2117.395783	17.949338	-0.049189	2.572788
258.116031	2109.415921	17.954343	-0.049163	2.568404
258.104679	2101.471620	17.959347	-0.049156	2.564040
258.098875	2093.521726	17.964352	-0.049149	2.559665
258.013793	2085.572219	17.969357	-0.049128	2.555277
258.003486	2077.583748	17.974362	-0.049121	2.550866
257.860567	2069.624185	17.979367	-0.049089	2.546453
257.667389	2061.690217	17.984371	-0.049048	2.542044
257.663749	2053.728089	17.989376	-0.049042	2.537624
257.564197	2045.736199	17.994381	-0.049018	2.533174
257.579002	2037.758973	17.999386	-0.049016	2.528731
257.351278	2029.814651	18.004391	-0.048968	2.524283
257.278948	2021.874392	18.009395	-0.048950	2.519839
257.208147	2013.916508	18.014400	-0.048931	2.515378
257.224122	2005.881869	18.019405	-0.048929	2.510872
257.381855	1997.900071	18.024410	-0.048953	2.506398
257.209067	1989.948840	18.029415	-0.048916	2.501910
257.196111	1981.991139	18.034419	-0.048908	2.497421
257.222993	1974.013905	18.039424	-0.048908	2.492916
257.088852	1966.046498	18.044429	-0.048878	2.488396
257.103354	1958.095885	18.049434	-0.048875	2.483889
257.063548	1950.137341	18.054439	-0.048862	2.479365
256.991173	1942.202496	18.059443	-0.048844	2.474844
256.900583	1934.232308	18.064448	-0.048822	2.470293
256.640810	1926.268003	18.069453	-0.048768	2.465725
256.891149	1918.302609	18.074458	-0.048809	2.461185
256.859844	1910.325367	18.079463	-0.048798	2.456609
256.760581	1902.370519	18.084467	-0.048775	2.452032
256.644061	1894.428499	18.089472	-0.048748	2.447453
256.458149	1886.462081	18.094477	-0.048708	2.442846
256.692829	1878.509355	18.099482	-0.048746	2.438270
256.457304	1870.533201	18.104487	-0.048697	2.433636
256.568642	1862.483443	18.109491	-0.048713	2.428977
256.510164	1854.537731	18.114496	-0.048697	2.424356
256.209277	1846.613464	18.119501	-0.048635	2.419721
256.296823	1838.669279	18.124506	-0.048646	2.415094
256.292974	1830.677081	18.129511	-0.048640	2.410424
256.056056	1822.747241	18.134515	-0.048591	2.405763
255.958028	1814.821389	18.139520	-0.048568	2.401107
256.015436	1806.857669	18.144525	-0.048573	2.396431
255.964886	1798.885154	18.149530	-0.048558	2.391732
255.761151	1790.920736	18.154535	-0.048515	2.387017
255.802929	1782.969208	18.159539	-0.048518	2.382319
255.774540	1775.019806	18.164544	-0.048507	2.377608
255.581274	1767.073302	18.169549	-0.048466	2.372876
255.733596	1759.080432	18.174554	-0.048489	2.368134
255.698242	1751.137298	18.179559	-0.048477	2.363398
255.646943	1743.199188	18.184563	-0.048463	2.358653
255.602806	1735.250566	18.189568	-0.048449	2.353894
255.614394	1727.241599	18.194573	-0.048446	2.349093
255.404416	1719.331862	18.199578	-0.048402	2.344324
255.194676	1711.376667	18.204583	-0.048357	2.339518
255.182189	1703.427516	18.209587	-0.048350	2.334722
255.314109	1695.432804	18.214592	-0.048369	2.329900
254.920084	1687.509252	18.219597	-0.048291	2.325068
254.854766	1679.579034	18.224602	-0.048273	2.320248
254.988160	1671.604927	18.229607	-0.048293	2.315409
254.882022	1663.638369	18.234611	-0.048268	2.310544
254.925514	1655.675866	18.239616	-0.048271	2.305684
254.782433	1647.732709	18.244621	-0.048239	2.300810
254.836152	1639.797555	18.249626	-0.048244	2.295947
254.882529	1631.804329	18.254631	-0.048247	2.291037
254.785497	1623.870677	18.259635	-0.048224	2.286141
254.753680	1615.942576	18.264640	-0.048213	2.281244
254.425890	1608.025157	18.269645	-0.048146	2.276317
254.487183	1599.999234	18.274650	-0.048152	2.271346
254.450519	1592.018916	18.279655	-0.048140	2.266384
254.449174	1584.074736	18.284659	-0.048135	2.261436
254.345824	1576.150071	18.289664	-0.048110	2.256481
254.155933	1568.212501	18.294669	-0.048070	2.251499
254.130239	1560.263833	18.299674	-0.048060	2.246514
253.934300	1552.340371	18.304679	-0.048018	2.241518
253.889480	1544.407201	18.309683	-0.048005	2.236519
253.935399	1536.432434	18.314688	-0.048008	2.231490
253.781922	1528.473137	18.319693	-0.047974	2.226441
253.745313	1520.544164	18.324698	-0.047962	2.221411
253.972151	1512.556501	18.329703	-0.047999	2.216356
253.840863	1504.619749	18.334707	-0.047969	2.211289
253.748380	1496.688973	18.339712	-0.047947	2.206218
253.517764	1488.777638	18.344717	-0.047899	2.201136
253.511711	1480.846281	18.349722	-0.047893	2.196049
253.400992	1472.871163	18.354727	-0.047867	2.190912
253.311615	1464.913733	18.359731	-0.047845	2.185777
253.354781	1456.977064	18.364736	-0.047848	2.180655
253.216270	1449.038244	18.369741	-0.047817	2.175503
253.060024	1441.113620	18.374746	-0.047782	2.170347
253.114813	1433.142475	18.379751	-0.047787	2.165167
253.191226	1425.197794	18.384755	-0.047796	2.159994
253.086694	1417.289016	18.389760	-0.047772	2.154816
252.862745	1409.329001	18.394765	-0.047725	2.149580
252.977620	1401.376224	18.399770	-0.047741	2.144367
252.853138	1393.456069	18.404775	-0.047712	2.139142
252.569699	1385.554243	18.409779	-0.047654	2.133900
252.658144	1377.592777	18.414784	-0.047666	2.128641
252.518972	1369.655609	18.419789	-0.047635	2.123364
252.610119	1361.730468	18.424794	-0.047646	2.118103
252.653393	1353.740599	18.429799	-0.047649	2.112782
252.450730	1345.784332	18.434803	-0.047606	2.107445
252.530122	1337.849521	18.439808	-0.047616	2.102137
252.308025	1329.936933	18.444813	-0.047569	2.096802
252.531807	1321.969212	18.449818	-0.047606	2.091458
252.186503	1314.077818	18.454823	-0.047536	2.086097
251.978501	1306.172512	18.459827	-0.047492	2.080727
252.137504	1298.231890	18.464832	-0.047517	2.075354
252.064323	1290.265272	18.469837	-0.047498	2.069927
251.989808	1282.343087	18.474842	-0.047479	2.064516
251.821409	1274.440362	18.479847	-0.047442	2.059094
251.782748	1266.506409	18.484851	-0.047430	2.053650
251.801935	1258.564634	18.489856	-0.047428	2.048192
251.863055	1250.610711	18.494861	-0.047434	2.042715
251.674839	1242.741010	18.499866	-0.047394	2.037256
251.570912	1234.794000	18.504871	-0.047369	2.031737
251.299749	1226.872822	18.509875	-0.047314	2.026204
251.620499	1218.910016	18.514880	-0.047368	2.020688
251.496524	1210.994766	18.519885	-0.047340	2.015144
251.226980	1203.105066	18.524890	-0.047284	2.009588
251.032930	1195.188058	18.529895	-0.047243	2.004005
251.052784	1187.257816	18.534899	-0.047242	1.998419
251.121365	1179.320421	18.539904	-0.047249	1.992817
250.823875	1171.405918	18.544909	-0.047189	1.987178
250.933768	1163.461889	18.549914	-0.047204	1.981544
250.732080	1155.564171	18.554919	-0.047161	1.975894
250.575014	1147.656793	18.559923	-0.047127	1.970226
250.773238	1139.693167	18.564928	-0.047158	1.964539
250.572358	1131.804006	18.569933	-0.047116	1.958846
250.547958	1123.874978	18.574938	-0.047106	1.953127
250.512322	1115.907685	18.579943	-0.047094	1.947363
250.528043	1107.990456	18.584947	-0.047092	1.941623
250.238420	1100.126372	18.589952	-0.047033	1.935871
250.227412	1092.166212	18.594957	-0.047025	1.930063
250.346780	1084.254669	18.599962	-0.047042	1.924287
250.423012	1076.339486	18.604967	-0.047051	1.918486
250.176105	1068.441656	18.609971	-0.047000	1.912644
250.135039	1060.529004	18.614976	-0.046987	1.906797
249.955272	1052.625420	18.619981	-0.046949	1.900922
249.746991	1044.755112	18.624986	-0.046905	1.895051
249.693458	1036.833583	18.629991	-0.046890	1.889141
249.846829	1028.885415	18.634995	-0.046913	1.883216
249.831058	1021.005897	18.640000	-0.046905	1.877304
249.472046	1013.108986	18.645005	-0.046833	1.871322
249.631779	1005.161815	18.650010	-0.046857	1.865342
249.672637	997.263452	18.655015	-0.046860	1.859365
249.365716	989.386537	18.660019	-0.046797	1.853346
249.309429	981.480932	18.665024	-0.046782	1.847314
249.120402	973.603565	18.670029	-0.046741	1.841268
249.302689	965.672069	18.675034	-0.046770	1.835205
249.228124	957.756842	18.680039	-0.046751	1.829104
249.262533	949.852097	18.685043	-0.046752	1.823003
249.172592	941.980826	18.690048	-0.046730	1.816893
248.875798	934.099623	18.695053	-0.046670	1.810730
248.875165	926.199355	18.700058	-0.046665	1.804566
248.875240	918.313584	18.705063	-0.046659	1.798393
248.675029	910.405507	18.710067	-0.046617	1.792156
248.661377	902.474638	18.715072	-0.046609	1.785903
248.591058	894.588581	18.720077	-0.046591	1.779656
248.618777	886.701654	18.725082	-0.046591	1.773398
248.262065	878.850849	18.730087	-0.046519	1.767099
248.265171	870.945193	18.735091	-0.046515	1.760779
248.524780	863.040692	18.740096	-0.046558	1.754469
248.481182	855.125181	18.745101	-0.046544	1.748089
248.273342	847.293343	18.750106	-0.046501	1.741733
248.147709	839.424939	18.755111	-0.046472	1.735334
247.881369	831.555433	18.760115	-0.046417	1.728893
247.758201	823.709013	18.765120	-0.046389	1.722464
247.885524	815.792394	18.770125	-0.046408	1.715986
247.873632	807.890300	18.775130	-0.046400	1.709478
247.879674	799.998845	18.780135	-0.046396	1.702956
247.814819	792.131089	18.785139	-0.046379	1.696419
247.751876	784.263626	18.790144	-0.046362	1.689857
247.444766	776.425445	18.795149	-0.046300	1.683262
247.389763	768.580010	18.800154	-0.046284	1.676669
247.549533	760.659687	18.805159	-0.046309	1.670014
247.472887	752.792377	18.810163	-0.046289	1.663347
247.309231	744.956879	18.815168	-0.046254	1.656668
247.349567	737.057829	18.820173	-0.046256	1.649935
247.253829	729.226220	18.825178	-0.046233	1.643213
247.003447	721.408047	18.830183	-0.046181	1.636455
246.960257	713.473147	18.835187	-0.046168	1.629596
246.942527	705.607256	18.840192	-0.046160	1.622771
246.758800	697.772522	18.845197	-0.046120	1.615922
246.778018	689.918860	18.850202	-0.046119	1.609055
246.716797	682.068442	18.855207	-0.046102	1.602151
246.708147	674.220290	18.860211	-0.046095	1.595226
246.612398	666.376910	18.865216	-0.046072	1.588262
246.411266	658.552189	18.870221	-0.046030	1.581269
246.269338	650.736132	18.875226	-0.045998	1.574262
246.367403	642.848078	18.880231	-0.046011	1.567193
246.122980	635.041582	18.885235	-0.045961	1.560116
246.216594	627.197655	18.890240	-0.045973	1.553022
245.975638	619.358849	18.895245	-0.045923	1.545851
245.760924	611.567339	18.900250	-0.045878	1.538694
245.961378	603.677417	18.905255	-0.045910	1.531474
245.855978	595.851969	18.910259	-0.045885	1.524234
245.829201	588.048262	18.915264	-0.045875	1.516992
245.876660	580.187302	18.920269	-0.045879	1.509673
245.883375	572.365806	18.925274	-0.045875	1.502348
245.806811	564.564837	18.930279	-0.045855	1.494995
245.534231	556.778956	18.935283	-0.045800	1.487589
245.638779	548.954984	18.940288	-0.045814	1.480168
245.467054	541.149098	18.945293	-0.045777	1.472684
245.296997	533.323378	18.950298	-0.045740	1.465143
245.347824	525.510986	18.955303	-0.045744	1.457610
245.224924	517.707664	18.960307	-0.045716	1.450020
244.892438	509.963769	18.965312	-0.045649	1.442414
244.634057	502.200704	18.970317	-0.045596	1.434761
244.808127	494.356467	18.975322	-0.045623	1.427057
244.588666	486.596297	18.980327	-0.045577	1.419330
244.551929	478.793982	18.985331	-0.045565	1.411548
244.369380	471.041815	18.990336	-0.045526	1.403750
244.267357	463.269138	18.995341	-0.045502	1.395901
244.347175	455.444742	19.000346	-0.045512	1.387985
244.303151	447.666068	19.005351	-0.045499	1.380050
244.170187	439.908583	19.010355	-0.045469	1.372076
244.051631	432.159124	19.015360	-0.045442	1.364065
243.948074	424.405742	19.020365	-0.045417	1.356006
244.140252	416.597509	19.025370	-0.045448	1.347893
243.955869	408.875195	19.030375	-0.045408	1.339755
243.574534	401.165868	19.035379	-0.045332	1.331545
243.558691	393.419348	19.040384	-0.045324	1.323311
243.384471	385.682841	19.045389	-0.045287	1.315007
243.210142	377.835030	19.050394	-0.045249	1.306530
243.021811	370.132957	19.055399	-0.045209	1.298153
243.034939	362.387532	19.060403	-0.045206	1.289712
242.881357	354.690207	19.065408	-0.045173	1.281237
242.761523	346.984026	19.070413	-0.045145	1.272702
242.801359	339.250356	19.075418	-0.045148	1.264109
242.471088	331.599792	19.080423	-0.045081	1.255480
241.993667	323.947556	19.085427	-0.044987	1.246761
241.928712	316.265813	19.090432	-0.044970	1.238026
241.767003	308.554810	19.095437	-0.044935	1.229177
241.233428	300.935871	19.100442	-0.044830	1.220297
240.823943	293.297541	19.105447	-0.044749	1.211354
240.703171	285.612101	19.110451	-0.044722	1.202347
240.462227	277.964478	19.115456	-0.044672	1.193291
240.160298	270.307964	19.120461	-0.044611	1.184144
239.914784	262.678251	19.125466	-0.044560	1.174969
239.531455	255.052130	19.130471	-0.044483	1.165697
239.296103	247.430898	19.135475	-0.044435	1.156388
238.993655	239.773020	19.140480	-0.044373	1.146944
238.490581	232.196939	19.145485	-0.044275	1.137480
238.088377	224.604213	19.150490	-0.044195	1.127937
237.716607	217.028958	19.155495	-0.044120	1.118342
237.422766	209.419422	19.160499	-0.044061	1.108636
236.841284	201.887239	19.165504	-0.043948	1.098880
236.468988	194.305188	19.170509	-0.043873	1.089019
236.158108	186.743354	19.175514	-0.043810	1.079108
235.591208	179.214201	19.180519	-0.043700	1.069089
234.950177	171.704718	19.185523	-0.043576	1.058985
234.842681	164.126167	19.190528	-0.043551	1.048814
234.391094	156.623008	19.195533	-0.043462	1.038565
233.832819	149.144655	19.200538	-0.043353	1.028222
233.458162	141.645549	19.205543	-0.043278	1.017789
232.961209	134.169812	19.210547	-0.043181	1.007251
232.454612	126.735780	19.215552	-0.043081	0.996658
231.665702	119.294277	19.220557	-0.042930	0.985870
231.309985	111.840692	19.225562	-0.042858	0.975054
230.866212	104.402857	19.230567	-0.042771	0.964116
230.277569	97.023234	19.235571	-0.042656	0.953102
229.815954	89.619228	19.240576	-0.042566	0.941956
229.320896	82.241914	19.245581	-0.042469	0.930707
228.829453	74.887259	19.250586	-0.042372	0.919356
228.237481	67.552640	19.255591	-0.042257	0.907866
227.862429	60.432274	19.260595	-0.042183	0.896627