Tue Mar 23 10:42:37 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.810224	0.010492	0.000000	0.000003	0.721130

0.944290	-0.017566	0.005005	-0.000022	0.721121
1.140420	-0.047233	0.010010	-0.000059	0.721132
0.891084	-0.008101	0.015014	-0.000012	0.721121
0.938150	-0.014839	0.020019	-0.000021	0.721125
1.134307	-0.048715	0.025024	-0.000057	0.721127
0.966779	-0.020737	0.030029	-0.000026	0.721123
0.919222	-0.007534	0.035034	-0.000017	0.721132
0.853370	-0.000237	0.040038	-0.000005	0.721124
0.835474	0.005028	0.045043	-0.000002	0.721128
0.781315	0.014567	0.050048	0.000008	0.721127
0.761314	0.014296	0.055053	0.000012	0.721120
0.911561	-0.007202	0.060058	-0.000016	0.721130
0.842718	-0.000642	0.065062	-0.000003	0.721119
0.873333	-0.004966	0.070067	-0.000009	0.721121
0.858135	-0.108135	0.075072	-0.000006	0.720913
0.954790	-0.145273	0.080077	-0.000024	0.720873
0.978692	-0.146261	0.085082	-0.000028	0.720880
0.985634	-0.150812	0.090086	-0.000029	0.720873
1.043102	-0.158728	0.095091	-0.000040	0.720878
1.142592	-0.177021	0.100096	-0.000059	0.720877
0.920380	-0.242345	0.105101	-0.000017	0.720670
1.098340	-0.338028	0.110106	-0.000050	0.720544
1.129744	-0.346299	0.115110	-0.000056	0.720539
0.959702	-0.312203	0.120115	-0.000024	0.720546
0.976133	-0.317253	0.125120	-0.000027	0.720542
0.844511	-0.412207	0.130125	-0.000003	0.720309
0.900034	-0.462448	0.135130	-0.000013	0.720229
0.966287	-0.478428	0.140134	-0.000025	0.720221
1.136306	-0.507060	0.145139	-0.000057	0.720224
0.882440	-0.551878	0.150144	-0.000010	0.720047
0.727630	-0.601086	0.155149	0.000019	0.719895
0.804378	-0.610459	0.160154	0.000005	0.719904
0.873914	-0.626111	0.165158	-0.000008	0.719897
0.827688	-0.728602	0.170163	0.000001	0.719679
0.887855	-0.776944	0.175168	-0.000010	0.719605
0.918438	-0.787282	0.180173	-0.000016	0.719595
0.830369	-0.830239	0.185178	0.000000	0.719479
0.830979	-0.938197	0.190182	0.000000	0.719267
0.905154	-0.947867	0.195187	-0.000014	0.719274
0.917727	-0.989335	0.200192	-0.000016	0.719196
0.864897	-1.101141	0.205197	-0.000006	0.718957
0.864855	-1.096689	0.210202	-0.000006	0.718966
0.806822	-1.149015	0.215206	0.000005	0.718842
0.663389	-1.222096	0.220211	0.000032	0.718647
0.732633	-1.234806	0.225216	0.000019	0.718647
0.789590	-1.335442	0.230221	0.000008	0.718468
0.756878	-1.382908	0.235226	0.000015	0.718362
0.644060	-1.367781	0.240230	0.000036	0.718353
0.516554	-1.509474	0.245235	0.000059	0.718028
0.636621	-1.534749	0.250240	0.000037	0.718020
0.589254	-1.596433	0.255245	0.000046	0.717881
0.712181	-1.704379	0.260250	0.000023	0.717711
0.603625	-1.696835	0.265254	0.000043	0.717688
0.535267	-1.837306	0.270259	0.000056	0.717386
0.481228	-1.829127	0.275264	0.000066	0.717383
0.439843	-1.931855	0.280269	0.000074	0.717165
0.440550	-1.969161	0.285274	0.000074	0.717092
0.471715	-2.054046	0.290278	0.000068	0.716935
0.445266	-2.138628	0.295283	0.000073	0.716758
0.211439	-2.138599	0.300288	0.000117	0.716676
-0.053075	-2.205183	0.305293	0.000166	0.716450
0.270098	-2.271668	0.310298	0.000106	0.716433
-0.025727	-2.368050	0.315302	0.000161	0.716137
-0.220002	-2.333079	0.320307	0.000197	0.716138
-1.526931	-2.217461	0.325312	0.000441	0.715906
-2.862147	-1.991647	0.330317	0.000689	0.715882
-2.967716	-1.968420	0.335322	0.000709	0.715891
-2.977037	-2.118576	0.340326	0.000711	0.715590
-3.945034	-1.964925	0.345331	0.000891	0.715552
-3.815547	-1.988877	0.350336	0.000867	0.715551
-3.466664	-2.113135	0.355341	0.000802	0.715427
-4.638157	-1.998609	0.360346	0.001020	0.715241
-4.666594	-1.999036	0.365350	0.001025	0.715230
-4.843515	-1.965148	0.370355	0.001058	0.715234
-4.483561	-2.084625	0.375360	0.000991	0.715125
-5.816298	-1.956784	0.380365	0.001239	0.714907
-5.310826	-2.042595	0.385370	0.001145	0.714915
-5.434122	-2.024628	0.390374	0.001168	0.714907
-5.648341	-1.984019	0.395379	0.001208	0.714912
-5.938887	-2.072940	0.400384	0.001262	0.714633
-6.601277	-1.969559	0.405389	0.001386	0.714604
-6.525044	-1.977699	0.410394	0.001371	0.714615
-6.635943	-1.965239	0.415398	0.001392	0.714600
-6.789081	-1.933899	0.420403	0.001421	0.714608
-6.924166	-2.050918	0.425408	0.001446	0.714328
-7.869817	-1.911724	0.430413	0.001622	0.714270
-7.516505	-1.968121	0.435418	0.001556	0.714283
-7.278401	-2.016842	0.440422	0.001512	0.714270
-7.370485	-1.996496	0.445427	0.001529	0.714278
-7.512050	-2.012663	0.450432	0.001555	0.714196
-8.473370	-1.957962	0.455437	0.001734	0.713964
-7.965716	-2.041934	0.460442	0.001640	0.713977
-8.736258	-1.911770	0.465446	0.001783	0.713963
-8.588630	-1.935263	0.470451	0.001756	0.713968
-8.093496	-2.020971	0.475456	0.001664	0.713973
-8.630275	-1.973041	0.480461	0.001764	0.713878
-9.198536	-1.982489	0.485466	0.001869	0.713658
-8.999995	-2.022824	0.490470	0.001833	0.713648
-9.626018	-1.910234	0.495475	0.001949	0.713650
-9.389086	-1.951678	0.500480	0.001905	0.713652
-9.393826	-1.953172	0.505485	0.001906	0.713647
-9.283835	-1.965685	0.510490	0.001885	0.713661
-9.783745	-2.010615	0.515494	0.001979	0.713395
-10.291683	-1.937103	0.520499	0.002073	0.713361
-9.782037	-2.028030	0.525504	0.001978	0.713361
-10.118955	-1.971606	0.530509	0.002041	0.713353
-10.427797	-1.911868	0.535514	0.002098	0.713363
-10.184621	-1.958661	0.540518	0.002053	0.713356
-10.208599	-2.032389	0.545523	0.002058	0.713201
-11.410555	-1.905547	0.550528	0.002281	0.713027
-11.059531	-1.972532	0.555533	0.002216	0.713018
-11.089784	-1.962266	0.560538	0.002222	0.713028
-11.477207	-1.898096	0.565542	0.002294	0.713018
-11.117524	-1.959567	0.570547	0.002227	0.713023
-10.974678	-1.983861	0.575552	0.002200	0.713025
-11.425589	-1.980516	0.580557	0.002284	0.712872
-12.077674	-1.943470	0.585562	0.002406	0.712715
-11.857750	-1.987335	0.590566	0.002365	0.712705
-12.188768	-1.928546	0.595571	0.002427	0.712705
-12.176598	-1.927916	0.600576	0.002424	0.712710
-12.340810	-1.904330	0.605581	0.002455	0.712699
-12.033850	-1.954334	0.610586	0.002398	0.712708
-12.324241	-1.942440	0.615590	0.002452	0.712629
-13.079887	-1.931768	0.620595	0.002593	0.712382
-12.724598	-1.991874	0.625600	0.002526	0.712388
-13.342134	-1.887368	0.630605	0.002641	0.712377
-13.301935	-1.888716	0.635610	0.002634	0.712389
-13.021866	-1.942668	0.640614	0.002582	0.712381
-13.324846	-1.885779	0.645619	0.002638	0.712387
-12.862129	-1.968704	0.650624	0.002552	0.712386
-13.539075	-1.971380	0.655629	0.002678	0.712140
-13.976995	-1.918486	0.660634	0.002760	0.712090
-14.071773	-1.905736	0.665638	0.002777	0.712081
-14.013336	-1.912607	0.670643	0.002767	0.712088
-13.987353	-1.916750	0.675648	0.002762	0.712089
-14.134301	-1.892944	0.680653	0.002789	0.712085
-13.715936	-1.964211	0.685658	0.002711	0.712091
-14.031618	-1.996394	0.690662	0.002770	0.711915
-14.873898	-1.924288	0.695667	0.002927	0.711759
-14.706532	-1.952720	0.700672	0.002896	0.711762
-15.233803	-1.861938	0.705677	0.002994	0.711756
-14.676457	-1.956364	0.710682	0.002890	0.711765
-14.795908	-1.939568	0.715686	0.002912	0.711756
-14.792119	-1.939679	0.720691	0.002912	0.711758
-14.466389	-2.079908	0.725696	0.002851	0.711594
-15.903425	-1.898750	0.730701	0.003119	0.711444
-15.487513	-1.968217	0.735706	0.003041	0.711453
-15.782604	-1.917740	0.740710	0.003096	0.711449
-15.742221	-1.923981	0.745715	0.003089	0.711451
-15.525809	-1.960565	0.750720	0.003048	0.711455
-15.902294	-1.898403	0.755725	0.003119	0.711445
-15.617214	-2.053605	0.760730	0.003066	0.711237
-16.809271	-1.893488	0.765734	0.003287	0.711132
-16.946666	-1.868759	0.770739	0.003313	0.711133
-16.490095	-1.947233	0.775744	0.003228	0.711138
-16.769444	-1.900654	0.780749	0.003280	0.711132
-16.550985	-1.934828	0.785754	0.003239	0.711142
-16.519744	-1.943858	0.790758	0.003234	0.711135
-16.478371	-2.017598	0.795763	0.003226	0.711002
-17.261791	-1.943515	0.800768	0.003372	0.710871
-17.404230	-1.924101	0.805773	0.003398	0.710859
-17.034996	-1.984477	0.810778	0.003330	0.710870
-17.538291	-1.898621	0.815782	0.003423	0.710862
-17.609224	-1.883348	0.820787	0.003437	0.710868
-17.130424	-1.966607	0.825792	0.003347	0.710872
-17.762324	-1.996555	0.830797	0.003465	0.710587
-18.404780	-1.907661	0.835802	0.003585	0.710536
-18.553395	-1.885659	0.840806	0.003612	0.710527
-18.214792	-1.945308	0.845811	0.003549	0.710528
-18.189457	-1.947619	0.850816	0.003545	0.710533
-18.777140	-1.845824	0.855821	0.003654	0.710527
-18.198871	-1.944035	0.860826	0.003546	0.710536
-18.378379	-2.001248	0.865830	0.003580	0.710358
-19.655661	-1.846091	0.870835	0.003818	0.710213
-19.311781	-1.904457	0.875840	0.003754	0.710219
-19.371284	-1.897041	0.880845	0.003765	0.710213
-19.684456	-1.836071	0.885850	0.003823	0.710223
-19.567033	-1.861078	0.890854	0.003801	0.710215
-19.523414	-1.867155	0.895859	0.003793	0.710218
-19.240301	-1.916255	0.900864	0.003741	0.710221
-19.975089	-1.929328	0.905869	0.003877	0.709933
-20.365231	-1.877946	0.910874	0.003950	0.709897
-20.046043	-1.936130	0.915878	0.003891	0.709894
-20.454389	-1.864331	0.920883	0.003967	0.709892
-20.391237	-1.871274	0.925888	0.003955	0.709901
-20.461734	-1.864552	0.930893	0.003968	0.709889
-20.318592	-1.885436	0.935898	0.003941	0.709898
-20.613472	-1.863279	0.940902	0.003996	0.709837
-21.141592	-1.891207	0.945907	0.004095	0.709593
-20.626996	-1.979841	0.950912	0.003999	0.709599
-21.670826	-1.797226	0.955917	0.004193	0.709592
-21.155565	-1.885822	0.960922	0.004097	0.709599
-20.852424	-1.943059	0.965926	0.004041	0.709592
-21.586947	-1.812008	0.970931	0.004178	0.709593
-21.144995	-1.889414	0.975936	0.004095	0.709595
-21.887436	-1.926017	0.980941	0.004234	0.709257
-21.978486	-1.904124	0.985946	0.004251	0.709269
-22.260117	-1.854042	0.990950	0.004303	0.709268
-22.009618	-1.899910	0.995955	0.004256	0.709266
-21.957948	-1.908438	1.000960	0.004247	0.709267
-22.541532	-1.807476	1.005965	0.004355	0.709261
-22.222196	-1.861126	1.010970	0.004296	0.709268
-22.033699	-1.982807	1.015974	0.004261	0.709091
-23.613776	-1.770421	1.020979	0.004555	0.708953
-22.915125	-1.891352	1.025984	0.004425	0.708960
-23.019851	-1.874936	1.030989	0.004445	0.708955
-22.882625	-1.897424	1.035994	0.004419	0.708959
-23.000558	-1.878147	1.040998	0.004441	0.708956
-23.192995	-1.845517	1.046003	0.004477	0.708952
-22.957749	-1.937458	1.051008	0.004433	0.708852
-24.296710	-1.808405	1.056013	0.004682	0.708633
-23.918703	-1.870568	1.061018	0.004612	0.708643
-23.903241	-1.874554	1.066022	0.004609	0.708640
-23.915935	-1.871731	1.071027	0.004612	0.708642
-23.806350	-1.890658	1.076032	0.004591	0.708643
-24.197849	-1.824891	1.081037	0.004664	0.708635
-23.979779	-1.858904	1.086042	0.004624	0.708644
-24.601540	-1.890171	1.091046	0.004739	0.708360
-24.946351	-1.834474	1.096051	0.004804	0.708348
-24.573423	-1.898421	1.101056	0.004734	0.708353
-24.880246	-1.849454	1.106061	0.004791	0.708342
-24.910127	-1.839635	1.111066	0.004797	0.708351
-24.623109	-1.893647	1.116070	0.004743	0.708345
-24.736660	-1.873669	1.121075	0.004765	0.708344
-25.215773	-1.936947	1.126080	0.004854	0.708046
-26.004814	-1.818234	1.131085	0.005001	0.708002
-25.622720	-1.881327	1.136090	0.004930	0.708012
-25.772633	-1.857126	1.141094	0.004958	0.708007
-26.072208	-1.803686	1.146099	0.005013	0.708007
-25.514633	-1.899023	1.151104	0.004910	0.708015
-25.795543	-1.855487	1.156109	0.004962	0.708002
-26.046674	-1.899324	1.161114	0.005009	0.707824
-26.925879	-1.808220	1.166118	0.005172	0.707693
-26.496406	-1.884117	1.171123	0.005092	0.707694
-26.418077	-1.894948	1.176128	0.005078	0.707700
-26.938880	-1.804339	1.181133	0.005175	0.707696
-26.221763	-1.928695	1.186138	0.005041	0.707703
-26.635154	-1.857500	1.191142	0.005118	0.707698
-26.759311	-1.916457	1.196147	0.005142	0.707535
-27.328249	-1.892553	1.201152	0.005247	0.707379
-27.216216	-1.916546	1.206157	0.005227	0.707371
-27.504852	-1.859843	1.211162	0.005280	0.707382
-27.528985	-1.858715	1.216166	0.005285	0.707375
-27.621464	-1.843113	1.221171	0.005302	0.707374
-27.570344	-1.849913	1.226176	0.005293	0.707378
-27.737406	-1.898036	1.231181	0.005324	0.707222
-28.252696	-1.873199	1.236186	0.005420	0.707087
-28.369402	-1.855805	1.241190	0.005441	0.707080
-28.705166	-1.795135	1.246195	0.005504	0.707082
-28.192763	-1.884688	1.251200	0.005409	0.707086
-28.578607	-1.820767	1.256205	0.005480	0.707076
-28.565422	-1.818282	1.261210	0.005478	0.707086
-28.435902	-1.875821	1.266214	0.005454	0.707016
-29.126813	-1.885708	1.271219	0.005583	0.706749
-29.160528	-1.876926	1.276224	0.005589	0.706755
-29.607760	-1.801944	1.281229	0.005672	0.706745
-29.049280	-1.893729	1.286234	0.005568	0.706761
-29.225448	-1.866590	1.291238	0.005601	0.706752
-29.479345	-1.822801	1.296243	0.005648	0.706749
-28.817289	-1.982184	1.301248	0.005525	0.706666
-30.197777	-1.849495	1.306253	0.005782	0.706438
-30.318949	-1.823768	1.311258	0.005805	0.706446
-30.310312	-1.829058	1.316262	0.005803	0.706439
-30.228240	-1.843669	1.321267	0.005788	0.706439
-30.145453	-1.854137	1.326272	0.005772	0.706447
-30.556995	-1.786988	1.331277	0.005849	0.706435
-30.155371	-1.850746	1.336282	0.005774	0.706450
-30.648259	-1.906367	1.341286	0.005866	0.706162
-31.384339	-1.791656	1.346291	0.006003	0.706129
-30.973840	-1.861038	1.351296	0.005927	0.706136
-30.829750	-1.893495	1.356301	0.005900	0.706123
-31.154042	-1.831141	1.361306	0.005960	0.706132
-31.133617	-1.836861	1.366310	0.005957	0.706128
-30.847518	-1.886477	1.371315	0.005903	0.706130
-31.275571	-1.926233	1.376320	0.005983	0.705897
-32.076682	-1.802213	1.381325	0.006132	0.705859
-31.701476	-1.865966	1.386330	0.006062	0.705865
-31.715388	-1.866497	1.391334	0.006065	0.705859
-32.207093	-1.779969	1.396339	0.006156	0.705857
-31.864048	-1.838418	1.401344	0.006093	0.705862
-31.764454	-1.875201	1.406349	0.006074	0.705824
-32.648196	-1.865674	1.411354	0.006239	0.705526
-32.747031	-1.850369	1.416358	0.006257	0.705522
-32.925032	-1.817580	1.421363	0.006290	0.705524
-32.545025	-1.882426	1.426368	0.006220	0.705530
-32.863635	-1.830082	1.431373	0.006279	0.705521
-32.753277	-1.847254	1.436378	0.006258	0.705526
-32.668641	-1.889116	1.441382	0.006243	0.705472
-33.733605	-1.830698	1.446387	0.006441	0.705207
-33.653648	-1.841019	1.451392	0.006426	0.705215
-33.627347	-1.849528	1.456397	0.006421	0.705207
-33.729450	-1.827670	1.461402	0.006440	0.705214
-33.864792	-1.806709	1.466406	0.006465	0.705208
-33.800312	-1.817915	1.471411	0.006453	0.705209
-33.470517	-1.872224	1.476416	0.006392	0.705218
-34.370909	-1.874621	1.481421	0.006560	0.704889
-34.551691	-1.843661	1.486426	0.006593	0.704887
-34.645326	-1.826335	1.491430	0.006611	0.704888
-34.547940	-1.844337	1.496435	0.006593	0.704887
-34.514743	-1.847991	1.501440	0.006587	0.704891
-34.617288	-1.833687	1.506445	0.006606	0.704883
-34.226545	-1.904210	1.511450	0.006533	0.704882
-34.837078	-1.941616	1.516454	0.006647	0.704587
-35.391327	-1.841413	1.521459	0.006750	0.704590
-35.472975	-1.825179	1.526464	0.006765	0.704593
-35.529151	-1.819642	1.531469	0.006776	0.704584
-35.223957	-1.869147	1.536474	0.006719	0.704594
-35.024259	-1.907050	1.541478	0.006682	0.704589
-35.344829	-1.920011	1.546483	0.006741	0.704448
-36.245301	-1.851690	1.551488	0.006909	0.704262
-36.125236	-1.875515	1.556493	0.006887	0.704257
-36.019042	-1.891332	1.561498	0.006867	0.704263
-36.386505	-1.828177	1.566502	0.006935	0.704258
-36.309648	-1.841512	1.571507	0.006921	0.704259
-35.941541	-1.905370	1.576512	0.006853	0.704263
-36.611261	-1.869100	1.581517	0.006977	0.704095
-37.271778	-1.821140	1.586522	0.007100	0.703954
-36.716122	-1.923886	1.591526	0.006997	0.703947
-37.005629	-1.872651	1.596531	0.007051	0.703946
-36.974081	-1.874042	1.601536	0.007045	0.703954
-36.959197	-1.879774	1.606541	0.007042	0.703948
-36.983402	-1.872001	1.611546	0.007047	0.703955
-37.445091	-1.911523	1.616550	0.007133	0.703709
-38.249737	-1.806780	1.621555	0.007282	0.703631
-38.012018	-1.845737	1.626560	0.007238	0.703638
-38.346668	-1.789973	1.631565	0.007300	0.703630
-38.345462	-1.787272	1.636570	0.007300	0.703636
-37.985845	-1.852637	1.641574	0.007233	0.703633
-38.071953	-1.838393	1.646579	0.007249	0.703631
-38.172894	-1.858275	1.651584	0.007268	0.703555
-39.067504	-1.807215	1.656589	0.007435	0.703336
-38.463552	-1.912464	1.661594	0.007322	0.703341
-38.929520	-1.831664	1.666598	0.007409	0.703336
-38.889836	-1.839148	1.671603	0.007402	0.703335
-38.480222	-1.909445	1.676608	0.007326	0.703341
-38.854733	-1.846031	1.681613	0.007395	0.703334
-38.993267	-1.902165	1.686618	0.007421	0.703170
-39.788212	-1.842500	1.691622	0.007569	0.703005
-39.771039	-1.846202	1.696627	0.007566	0.703003
-39.690864	-1.857774	1.701632	0.007551	0.703009
-40.025570	-1.801916	1.706637	0.007613	0.703001
-39.720277	-1.852577	1.711642	0.007557	0.703009
-39.923778	-1.818293	1.716646	0.007594	0.703005
-40.353060	-1.770026	1.721651	0.007674	0.702947
-40.425555	-1.882755	1.726656	0.007688	0.702693
-40.236698	-1.921156	1.731661	0.007653	0.702684
-40.883402	-1.800988	1.736666	0.007773	0.702694
-40.724276	-1.833085	1.741670	0.007744	0.702686
-40.762013	-1.825261	1.746675	0.007751	0.702688
-40.849914	-1.806718	1.751680	0.007767	0.702694
-40.904839	-1.806602	1.756685	0.007777	0.702675
-41.042039	-1.933218	1.761690	0.007803	0.702369
-41.486003	-1.854480	1.766694	0.007885	0.702368
-41.851893	-1.790548	1.771699	0.007954	0.702366
-41.267394	-1.890101	1.776704	0.007845	0.702375
-41.795758	-1.800485	1.781709	0.007943	0.702366
-41.839448	-1.790133	1.786714	0.007951	0.702371
-41.688975	-1.819760	1.791718	0.007923	0.702365
-42.198213	-1.863431	1.796723	0.008018	0.702093
-42.797860	-1.764420	1.801728	0.008130	0.702077
-42.889338	-1.753188	1.806733	0.008147	0.702067
-42.148622	-1.881560	1.811738	0.008009	0.702074
-42.518007	-1.816502	1.816742	0.008078	0.702073
-42.634631	-1.798048	1.821747	0.008100	0.702068
-42.225375	-1.867946	1.826752	0.008023	0.702074
-42.723015	-1.894343	1.831757	0.008116	0.701841
-43.732159	-1.762386	1.836762	0.008304	0.701744
-43.382357	-1.827355	1.841766	0.008239	0.701739
-43.234249	-1.853513	1.846771	0.008211	0.701739
-43.248904	-1.847723	1.851776	0.008214	0.701745
-43.440966	-1.818286	1.856781	0.008250	0.701736
-43.069048	-1.880875	1.861786	0.008181	0.701743
-43.413977	-1.930084	1.866790	0.008245	0.701519
-44.284933	-1.816956	1.871795	0.008407	0.701434
-43.973648	-1.869509	1.876800	0.008349	0.701440
-44.172038	-1.837553	1.881805	0.008386	0.701433
-44.356848	-1.801004	1.886810	0.008420	0.701440
-44.175670	-1.834870	1.891814	0.008387	0.701437
-43.996440	-1.873360	1.896819	0.008353	0.701423
-44.804309	-1.876769	1.901824	0.008504	0.701125
-45.249474	-1.802047	1.906829	0.008587	0.701115
-45.075256	-1.829009	1.911834	0.008554	0.701124
-44.918345	-1.858895	1.916838	0.008525	0.701120
-45.204347	-1.808928	1.921843	0.008578	0.701117
-44.984692	-1.845763	1.926848	0.008537	0.701122
-44.805706	-1.891411	1.931853	0.008504	0.701094
-45.628760	-1.852915	1.936858	0.008657	0.700875
-45.755502	-1.831034	1.941862	0.008681	0.700873
-45.964450	-1.795613	1.946867	0.008720	0.700870
-45.378040	-1.897493	1.951872	0.008611	0.700875
-45.823103	-1.821938	1.956877	0.008694	0.700867
-45.693171	-1.842084	1.961882	0.008669	0.700873
-45.892782	-1.899463	1.966886	0.008707	0.700685
-47.001859	-1.777842	1.971891	0.008913	0.700531
-46.240829	-1.909935	1.976896	0.008772	0.700538
-46.186226	-1.923850	1.981901	0.008761	0.700529
-46.545301	-1.857195	1.986906	0.008828	0.700535
-46.568550	-1.853111	1.991910	0.008833	0.700534
-46.452456	-1.905354	1.996915	0.008811	0.700470
-47.363286	-1.865946	2.001920	0.008981	0.700221

-47.431229	-1.852221	2.011917	0.008993	0.700224
-47.661591	-1.812888	2.021914	0.009036	0.700221
-47.395852	-1.860970	2.031910	0.008987	0.700219
-47.409422	-1.858942	2.041907	0.008989	0.700218
-47.486589	-1.846038	2.051904	0.009004	0.700216
-47.407407	-1.859739	2.061901	0.008989	0.700217
-47.550851	-1.835210	2.071898	0.009016	0.700215
-47.303786	-1.880271	2.081894	0.008970	0.700213
-47.439062	-1.856505	2.091891	0.008995	0.700212
-47.486650	-1.846332	2.101888	0.009004	0.700215
-47.338318	-1.872016	2.111885	0.008976	0.700217
-47.505583	-1.841237	2.121882	0.009007	0.700219
-47.373845	-1.867930	2.131878	0.008983	0.700212
-46.828132	-1.817098	2.141875	0.008881	0.700513
-46.594899	-1.848555	2.151872	0.008838	0.700533
-46.340870	-1.893739	2.161869	0.008791	0.700533
-46.362078	-1.890119	2.171866	0.008795	0.700533
-46.562932	-1.855740	2.181862	0.008832	0.700530
-45.965659	-1.812680	2.191859	0.008721	0.700833
-45.696817	-1.842267	2.201856	0.008671	0.700870
-45.580589	-1.861608	2.211853	0.008649	0.700873
-45.775769	-1.825698	2.221850	0.008686	0.700875
-45.116344	-1.846752	2.231846	0.008563	0.701071
-45.189904	-1.807764	2.241843	0.008577	0.701123
-44.939654	-1.852388	2.251840	0.008530	0.701123
-44.736655	-1.876168	2.261837	0.008492	0.701148
-44.238027	-1.821783	2.271834	0.008400	0.701438
-44.009361	-1.864024	2.281830	0.008357	0.701435
-44.180641	-1.832530	2.291827	0.008389	0.701437
-43.887442	-1.811791	2.301824	0.008334	0.701585
-43.043304	-1.882076	2.311821	0.008177	0.701747
-43.320051	-1.833208	2.321818	0.008229	0.701746
-43.293789	-1.832762	2.331814	0.008224	0.701756
-42.626514	-1.795951	2.341811	0.008100	0.702072
-42.176508	-1.876222	2.351808	0.008016	0.702071
-42.267931	-1.858038	2.361805	0.008033	0.702075
-42.058437	-1.826400	2.371802	0.007994	0.702215
-41.392898	-1.870676	2.381798	0.007870	0.702365
-41.561909	-1.842872	2.391795	0.007902	0.702360
-41.469349	-1.856366	2.401792	0.007884	0.702366
-40.831318	-1.817209	2.411789	0.007766	0.702675
-40.540595	-1.862742	2.421786	0.007712	0.702688
-40.574322	-1.857509	2.431782	0.007718	0.702686
-40.489134	-1.797653	2.441779	0.007702	0.702838
-39.447919	-1.902598	2.451776	0.007508	0.703001
-39.809636	-1.837543	2.461773	0.007576	0.703002
-39.722446	-1.853248	2.471770	0.007559	0.703002
-39.085640	-1.809660	2.481766	0.007441	0.703319
-39.018085	-1.813158	2.491763	0.007428	0.703336
-38.712165	-1.866847	2.501760	0.007371	0.703338
-38.739497	-1.783105	2.511757	0.007376	0.703497
-37.956685	-1.855529	2.521754	0.007231	0.703632
-38.248074	-1.804445	2.531750	0.007285	0.703631
-37.990021	-1.828074	2.541747	0.007237	0.703676
-37.088180	-1.852329	2.551744	0.007069	0.703951
-37.094333	-1.851084	2.561741	0.007070	0.703951
-36.872010	-1.892775	2.571738	0.007029	0.703947
-36.929402	-1.794691	2.581734	0.007040	0.704124
-36.344252	-1.833092	2.591731	0.006931	0.704257
-36.300674	-1.839820	2.601728	0.006923	0.704259
-36.078595	-1.861626	2.611725	0.006881	0.704295
-35.361481	-1.841112	2.621722	0.006748	0.704594
-35.525249	-1.812432	2.631718	0.006778	0.704593
-35.354128	-1.841894	2.641715	0.006747	0.704595
-34.968284	-1.817534	2.651712	0.006675	0.704783
-34.627368	-1.823387	2.661709	0.006611	0.704893
-34.291486	-1.885901	2.671706	0.006549	0.704888
-34.564564	-1.817645	2.681702	0.006600	0.704927
-33.721095	-1.827697	2.691699	0.006443	0.705210
-33.489692	-1.868716	2.701696	0.006400	0.705210
-33.666802	-1.834750	2.711693	0.006433	0.705215
-33.042211	-1.850836	2.721690	0.006316	0.705407
-32.761174	-1.843012	2.731686	0.006264	0.705523
-32.800933	-1.836166	2.741683	0.006272	0.705522
-32.578536	-1.869095	2.751680	0.006230	0.705536
-31.753529	-1.855757	2.761677	0.006077	0.705859
-31.585957	-1.883805	2.771674	0.006045	0.705862
-31.803335	-1.846390	2.781670	0.006086	0.705859
-31.624792	-1.847025	2.791667	0.006053	0.705922
-30.877135	-1.877867	2.801664	0.005914	0.706128
-30.921393	-1.871230	2.811661	0.005922	0.706125
-30.805632	-1.891869	2.821658	0.005900	0.706125
-30.336766	-1.857674	2.831654	0.005813	0.706362
-30.179542	-1.845700	2.841651	0.005784	0.706442
-30.141382	-1.851925	2.851648	0.005777	0.706444
-30.051875	-1.814967	2.861645	0.005760	0.706550
-29.246833	-1.859708	2.871642	0.005610	0.706748
-29.519536	-1.811348	2.881638	0.005661	0.706748
-29.264399	-1.838272	2.891635	0.005614	0.706785
-28.622796	-1.805948	2.901632	0.005494	0.707079
-28.035709	-1.909454	2.911629	0.005385	0.707082
-28.426068	-1.839661	2.921626	0.005458	0.707082
-28.055570	-1.812482	2.931622	0.005389	0.707269
-27.651862	-1.833089	2.941619	0.005313	0.707372
-27.676143	-1.827523	2.951616	0.005318	0.707374
-27.364937	-1.837399	2.961613	0.005260	0.707466
-26.746094	-1.831910	2.971610	0.005145	0.707698
-26.402185	-1.893750	2.981606	0.005081	0.707697
-26.493872	-1.877963	2.991603	0.005098	0.707696
-26.114314	-1.847169	3.001600	0.005027	0.707893
-25.563345	-1.886095	3.011597	0.004925	0.708012
-25.859361	-1.832143	3.021594	0.004980	0.708014
-25.677834	-1.847820	3.031590	0.004946	0.708048
-24.975302	-1.824509	3.041587	0.004815	0.708345
-24.693227	-1.872521	3.051584	0.004763	0.708350
-24.674392	-1.874793	3.061581	0.004759	0.708352
-24.515614	-1.825305	3.071578	0.004730	0.708508
-23.776869	-1.891978	3.081574	0.004592	0.708638
-23.962567	-1.860299	3.091571	0.004627	0.708635
-23.977049	-1.857063	3.101568	0.004630	0.708636
-23.118534	-1.851071	3.111565	0.004470	0.708955
-22.938018	-1.880748	3.121562	0.004436	0.708960
-22.862057	-1.896984	3.131558	0.004422	0.708954
-22.911058	-1.842756	3.141555	0.004431	0.709045
-21.942184	-1.906617	3.151552	0.004251	0.709263
-21.803357	-1.929683	3.161549	0.004225	0.709266
-22.122197	-1.874048	3.171546	0.004285	0.709264
-21.579098	-1.870713	3.181542	0.004183	0.709464
-21.363649	-1.844668	3.191539	0.004143	0.709593
-21.388173	-1.839017	3.201536	0.004148	0.709595
-20.913088	-1.901919	3.211533	0.004060	0.709639
-20.535978	-1.840542	3.221530	0.003989	0.709896
-20.308324	-1.882129	3.231526	0.003947	0.709894
-20.472161	-1.852436	3.241523	0.003978	0.709895
-19.845947	-1.855291	3.251520	0.003861	0.710112
-19.454543	-1.872771	3.261517	0.003788	0.710217
-19.436545	-1.875751	3.271514	0.003785	0.710217
-19.449926	-1.856367	3.281510	0.003787	0.710251
-18.774129	-1.837489	3.291507	0.003662	0.710529
-18.312902	-1.917562	3.301504	0.003576	0.710533
-18.571447	-1.871817	3.311501	0.003624	0.710533
-18.201952	-1.840954	3.321498	0.003555	0.710726
-17.467243	-1.900101	3.331494	0.003418	0.710869
-17.727605	-1.854033	3.341491	0.003467	0.710868
-17.286438	-1.930999	3.351488	0.003385	0.710871
-16.740023	-1.919471	3.361485	0.003283	0.711089
-16.744461	-1.893908	3.371482	0.003284	0.711138
-16.755879	-1.891959	3.381478	0.003286	0.711138
-16.774255	-1.853575	3.391475	0.003289	0.711208
-15.916159	-1.885340	3.401472	0.003130	0.711450
-15.909578	-1.885620	3.411469	0.003129	0.711451
-15.836810	-1.897299	3.421466	0.003115	0.711454
-15.283368	-1.870118	3.431462	0.003012	0.711705
-15.156427	-1.865312	3.441459	0.002988	0.711759
-14.959153	-1.901289	3.451456	0.002952	0.711758
-14.776385	-1.878446	3.461453	0.002918	0.711868
-13.837597	-1.933517	3.471450	0.002743	0.712092
-14.074498	-1.892340	3.481446	0.002787	0.712090
-14.058592	-1.896123	3.491443	0.002784	0.712088
-13.376549	-1.927808	3.501440	0.002657	0.712267
-13.253597	-1.889207	3.511437	0.002634	0.712387
-13.240712	-1.891314	3.521434	0.002632	0.712387
-13.183709	-1.887161	3.531430	0.002621	0.712416
-12.536539	-1.855067	3.541427	0.002501	0.712709
-12.093756	-1.933562	3.551424	0.002419	0.712710
-12.296877	-1.897306	3.561421	0.002456	0.712710
-11.794116	-1.897752	3.571418	0.002363	0.712887
-11.391292	-1.900471	3.581414	0.002288	0.713025
-11.172922	-1.940832	3.591411	0.002247	0.713022
-11.166633	-1.940586	3.601408	0.002246	0.713025
-10.740730	-1.888772	3.611405	0.002167	0.713279
-10.437715	-1.900773	3.621402	0.002110	0.713362
-10.453454	-1.897427	3.631398	0.002113	0.713363
-10.225219	-1.918060	3.641395	0.002071	0.713403
-9.576742	-1.907943	3.651392	0.001950	0.713653
-9.535195	-1.915391	3.661389	0.001943	0.713653
-9.583552	-1.907178	3.671386	0.001952	0.713652
-9.247336	-1.859589	3.681382	0.001889	0.713865
-8.736990	-1.897672	3.691379	0.001794	0.713970
-8.514738	-1.938292	3.701376	0.001753	0.713968
-8.480845	-1.930656	3.711373	0.001746	0.713995
-7.492257	-1.964645	3.721370	0.001562	0.714278
-7.572190	-1.949746	3.731366	0.001577	0.714279
-7.335407	-1.992521	3.741363	0.001533	0.714278
-7.583236	-1.933478	3.751360	0.001579	0.714307
-6.906546	-1.902321	3.761357	0.001453	0.714609
-6.407761	-1.990700	3.771354	0.001361	0.714609
-6.548668	-1.966357	3.781350	0.001387	0.714608
-6.558087	-1.921951	3.791347	0.001389	0.714693
-5.653293	-1.972947	3.801344	0.001220	0.714911
-5.493804	-2.002701	3.811341	0.001191	0.714909
-5.596867	-1.982383	3.821338	0.001210	0.714912
-5.422460	-1.925734	3.831334	0.001177	0.715086
-4.814865	-1.959492	3.841331	0.001064	0.715234
-4.971220	-1.931927	3.851328	0.001093	0.715233
-4.936002	-1.934230	3.861325	0.001087	0.715241
-4.095920	-1.929829	3.871322	0.000930	0.715547
-3.990284	-1.948534	3.881318	0.000911	0.715547
-3.862362	-1.972232	3.891315	0.000887	0.715545
-3.906596	-1.890708	3.901312	0.000895	0.715691
-2.785014	-1.992325	3.911309	0.000686	0.715886
-3.048401	-1.946093	3.921306	0.000736	0.715884
-3.051256	-1.946263	3.931302	0.000736	0.715883
-2.604675	-1.927511	3.941299	0.000653	0.716077
-2.250930	-1.961496	3.951296	0.000587	0.716135
-2.219089	-1.965913	3.961293	0.000581	0.716137
-2.250159	-1.903001	3.971290	0.000587	0.716251
-1.546358	-1.927716	3.981286	0.000456	0.716450
-1.714229	-1.897433	3.991283	0.000487	0.716451
-1.807261	-1.837113	4.001280	0.000505	0.716538
-1.169495	-1.838380	4.011277	0.000386	0.716760
-1.146250	-1.842646	4.021274	0.000382	0.716760
-1.067837	-1.785954	4.031270	0.000367	0.716899
-1.010780	-1.702304	4.041267	0.000356	0.717085
-1.093763	-1.684571	4.051264	0.000372	0.717091
-1.315572	-1.498692	4.061261	0.000413	0.717380
-1.238157	-1.496407	4.071258	0.000399	0.717412
-1.123318	-1.368082	4.081254	0.000377	0.717706
-0.861607	-1.376591	4.091251	0.000329	0.717781
-0.747582	-1.279402	4.101248	0.000307	0.718014
-0.509834	-1.239449	4.111245	0.000263	0.718176
-0.483748	-1.152962	4.121242	0.000258	0.718356
-0.560998	-1.022408	4.131238	0.000272	0.718587
-0.684517	-0.928982	4.141235	0.000295	0.718728
-0.602718	-0.825066	4.151232	0.000280	0.718962
-0.404963	-0.726193	4.161229	0.000243	0.719226
-0.351870	-0.634357	4.171226	0.000233	0.719426
-0.238206	-0.544560	4.181222	0.000212	0.719643
-0.224275	-0.419248	4.191219	0.000210	0.719895
-0.048200	-0.305192	4.201216	0.000177	0.720181
-0.093952	-0.173086	4.211213	0.000185	0.720425
0.076399	-0.068222	4.221210	0.000153	0.720692
0.026624	0.073384	4.231206	0.000163	0.720953
0.000000	0.224797	4.241203	0.000168	0.721241

-0.170477	0.877368	4.246208	0.000199	0.722464
0.079728	2.098843	4.251213	0.000152	0.724947
0.501047	3.875605	4.256218	0.000072	0.728562
0.788574	6.244379	4.261222	0.000017	0.733260
0.907358	9.134408	4.266227	-0.000007	0.738872
1.285792	12.468474	4.271232	-0.000080	0.745376
1.672577	16.256147	4.276237	-0.000154	0.752681
1.890276	20.467352	4.281242	-0.000197	0.760651
2.368155	25.042190	4.286246	-0.000289	0.769294
2.633827	30.016699	4.291251	-0.000342	0.778501
3.140188	35.294836	4.296256	-0.000440	0.788224
3.440744	40.935000	4.301261	-0.000499	0.798406
3.878265	46.840281	4.306266	-0.000585	0.808969
4.511855	53.007376	4.311270	-0.000707	0.819908
4.674299	59.520990	4.316275	-0.000741	0.831152
5.004558	66.227787	4.321280	-0.000807	0.842621
5.508866	73.125398	4.326285	-0.000905	0.854304
5.763329	80.265770	4.331290	-0.000957	0.866155
6.321463	87.551369	4.336294	-0.001066	0.878166
7.022540	94.976637	4.341299	-0.001201	0.890278
7.406194	102.620366	4.346304	-0.001278	0.902482
7.982758	110.387854	4.351309	-0.001390	0.914768
9.152698	118.150501	4.356314	-0.001613	0.927043
10.869127	125.982974	4.361318	-0.001938	0.939406
11.592131	134.088049	4.366323	-0.002078	0.951755
12.335278	142.281181	4.371328	-0.002221	0.964080
12.878933	150.597154	4.376333	-0.002328	0.976377
13.482293	158.974210	4.381338	-0.002446	0.988624
14.435060	167.358874	4.386342	-0.002629	1.000817
15.125331	175.809523	4.391347	-0.002763	1.012891
15.929684	184.299753	4.396352	-0.002918	1.024905
16.360908	192.893017	4.401357	-0.003004	1.036831
17.073561	201.454491	4.406362	-0.003142	1.048645
17.717557	210.068424	4.411366	-0.003268	1.060381
18.365974	218.691083	4.416371	-0.003394	1.072000
19.053117	227.318708	4.421376	-0.003528	1.083510
19.707344	235.963522	4.426381	-0.003655	1.094913
20.507839	244.571901	4.431386	-0.003810	1.106184
21.255810	253.208204	4.436390	-0.003954	1.117365
21.856785	261.847599	4.441395	-0.004072	1.128407
22.524034	270.497600	4.446400	-0.004202	1.139369
23.032265	279.178624	4.451405	-0.004302	1.150231
23.552562	287.830204	4.456410	-0.004405	1.160957
24.277196	296.436887	4.461414	-0.004545	1.171573
24.798414	305.049978	4.466419	-0.004648	1.182059
25.192553	313.693045	4.471424	-0.004727	1.192462
25.839790	322.261719	4.476429	-0.004853	1.202739
26.420049	330.837348	4.481434	-0.004967	1.212922
27.422802	339.344534	4.486438	-0.005159	1.223025
28.091335	347.909439	4.491443	-0.005289	1.233045
29.010013	356.396511	4.496448	-0.005465	1.242944
29.846921	364.910087	4.501453	-0.005627	1.252779
30.324285	373.448838	4.506458	-0.005721	1.262496
31.064992	381.963633	4.511462	-0.005865	1.272162
31.622657	390.459053	4.516467	-0.005974	1.281700
32.091083	398.978300	4.521472	-0.006067	1.291176
32.576263	407.478728	4.526477	-0.006163	1.300565
33.103923	415.995269	4.531482	-0.006266	1.309912
33.969818	424.478635	4.536486	-0.006433	1.319218
34.456313	432.888551	4.541491	-0.006529	1.328312
35.105447	441.298607	4.546496	-0.006656	1.337373
35.702045	449.689792	4.551501	-0.006772	1.346344
36.090071	458.122043	4.556506	-0.006850	1.355261
37.034729	466.440341	4.561510	-0.007031	1.364098
37.755934	474.806853	4.566515	-0.007171	1.372889
38.299381	483.187893	4.571520	-0.007277	1.381609
38.853167	491.578065	4.576525	-0.007386	1.390284
39.462479	499.932265	4.581530	-0.007505	1.398879
40.083164	508.269687	4.586534	-0.007626	1.407405
40.725185	516.606802	4.591539	-0.007751	1.415884
41.176893	524.948213	4.596544	-0.007840	1.424284
41.626816	533.313079	4.601549	-0.007930	1.432658
42.041690	541.630078	4.606554	-0.008012	1.440931
42.814159	549.922346	4.611558	-0.008161	1.449189
43.432044	558.230674	4.616563	-0.008282	1.457391
44.018876	566.529201	4.621568	-0.008397	1.465533
44.611057	574.878901	4.626573	-0.008512	1.473679
45.430725	583.119797	4.631578	-0.008670	1.481712
46.077714	591.392630	4.636582	-0.008796	1.489705
46.471533	599.700355	4.641587	-0.008875	1.497648
47.274908	607.915512	4.646592	-0.009030	1.505526
48.035912	616.177860	4.651597	-0.009177	1.513400
48.601412	624.425765	4.656602	-0.009287	1.521189
49.142508	632.704693	4.661606	-0.009394	1.528964
49.565118	640.986659	4.666611	-0.009478	1.536685
50.188417	649.232413	4.671616	-0.009599	1.544363
50.895109	657.477644	4.676621	-0.009736	1.552015
51.282232	665.743135	4.681626	-0.009813	1.559600
51.826930	673.978384	4.686630	-0.009920	1.567145
52.608263	682.183782	4.691635	-0.010071	1.574660
53.452798	690.362720	4.696640	-0.010234	1.582125
54.044435	698.602050	4.701645	-0.010349	1.589572
54.372144	706.871093	4.706650	-0.010416	1.596973
55.094533	715.061882	4.711654	-0.010555	1.604326
55.880622	723.255007	4.716659	-0.010707	1.611657
56.716687	731.447355	4.721664	-0.010868	1.618960
57.437930	739.646603	4.726669	-0.011008	1.626221
58.055232	747.925866	4.731674	-0.011128	1.633504
58.471352	756.151616	4.736678	-0.011211	1.640680
58.573069	764.403680	4.741683	-0.011235	1.647805
59.221541	772.590089	4.746688	-0.011361	1.654917
59.635041	780.786798	4.751693	-0.011443	1.661975
60.058980	788.975635	4.756698	-0.011528	1.668998
60.950211	797.120454	4.761702	-0.011699	1.676017
61.663914	805.260077	4.766707	-0.011837	1.682978
62.280132	813.445141	4.771712	-0.011957	1.689936
62.895034	821.637543	4.776717	-0.012077	1.696871
63.638320	829.781211	4.781722	-0.012221	1.703753
64.196645	837.997547	4.786726	-0.012330	1.710644
64.632859	846.204379	4.791731	-0.012417	1.717483
65.274671	854.349623	4.796736	-0.012541	1.724271
65.697736	862.544797	4.801741	-0.012625	1.731045
66.155099	870.723509	4.806746	-0.012716	1.737783
66.929642	878.854678	4.811750	-0.012865	1.744497
67.444284	887.028868	4.816755	-0.012967	1.751186
67.938210	895.214275	4.821760	-0.013064	1.757857
68.326834	903.385873	4.826765	-0.013142	1.764478
68.798584	911.559841	4.831770	-0.013235	1.771086
69.265498	919.737968	4.836774	-0.013327	1.777672
69.670963	927.897857	4.841779	-0.013408	1.784212
70.170396	936.081838	4.846784	-0.013506	1.790758
70.816405	944.251610	4.851789	-0.013632	1.797287
71.298492	952.361389	4.856794	-0.013727	1.803725
72.043409	960.483797	4.861798	-0.013871	1.810182
72.527086	968.618369	4.866803	-0.013966	1.816593
73.118047	976.733700	4.871808	-0.014081	1.822980
73.351338	984.924823	4.876813	-0.014130	1.829360
73.797301	993.076516	4.881818	-0.014218	1.835713
74.155914	1001.227861	4.886822	-0.014290	1.842033
74.405465	1009.386177	4.891827	-0.014342	1.848324
74.835282	1017.534542	4.896832	-0.014428	1.854607
75.324367	1025.647143	4.901837	-0.014524	1.860848
75.758031	1033.774512	4.906842	-0.014610	1.867073
76.313771	1041.937668	4.911846	-0.014719	1.873319
76.818368	1050.045848	4.916851	-0.014818	1.879496
77.183432	1058.168930	4.921856	-0.014891	1.885648
77.471270	1066.331661	4.926861	-0.014950	1.891801
77.864814	1074.446855	4.931866	-0.015029	1.897910
78.614316	1082.527964	4.936870	-0.015173	1.904015
78.909264	1090.672634	4.941875	-0.015234	1.910095
79.143746	1098.834086	4.946880	-0.015283	1.916162
79.765598	1106.920415	4.951885	-0.015404	1.922198
80.073319	1115.042201	4.956890	-0.015466	1.928205
80.690791	1123.165410	4.961894	-0.015587	1.934229
81.119874	1131.278635	4.966899	-0.015672	1.940207
81.127548	1139.457746	4.971904	-0.015678	1.946167
81.446815	1147.620880	4.976909	-0.015743	1.952132
82.027498	1155.703033	4.981914	-0.015857	1.958048
82.483362	1163.797403	4.986918	-0.015947	1.963942
82.702774	1171.913990	4.991923	-0.015993	1.969808
83.181711	1180.010428	4.996928	-0.016087	1.975670
83.636745	1188.119385	5.001933	-0.016177	1.981522
84.155811	1196.187762	5.006938	-0.016279	1.987333
84.573505	1204.330419	5.011942	-0.016362	1.993170
85.052621	1212.419006	5.016947	-0.016457	1.998957
85.824947	1220.453790	5.021952	-0.016606	2.004721
86.248117	1228.581259	5.026957	-0.016690	2.010496
86.442787	1236.719515	5.031962	-0.016731	2.016239
87.218696	1244.782089	5.036966	-0.016881	2.021972
87.476449	1252.917435	5.041971	-0.016934	2.027687
87.881753	1261.063461	5.046976	-0.017015	2.033408
88.512997	1269.144069	5.051981	-0.017138	2.039090
88.679797	1277.251138	5.056986	-0.017174	2.044728
89.159486	1285.348031	5.061990	-0.017269	2.050374
89.474162	1293.472056	5.066995	-0.017333	2.056007
89.869531	1301.559561	5.072000	-0.017411	2.061608
90.118996	1309.679045	5.077005	-0.017463	2.067201
90.386706	1317.794991	5.082010	-0.017518	2.072777
90.840079	1325.884250	5.087014	-0.017608	2.078339
91.192246	1333.953722	5.092019	-0.017679	2.083863
91.594285	1342.046190	5.097024	-0.017759	2.089392
92.038898	1350.155417	5.102029	-0.017847	2.094923
92.337715	1358.250081	5.107034	-0.017908	2.100414
92.835224	1366.328421	5.112038	-0.018006	2.105899
93.084686	1374.476813	5.117043	-0.018058	2.111393
93.637907	1382.571836	5.122048	-0.018166	2.116866
93.907019	1390.663585	5.127053	-0.018221	2.122296
94.138572	1398.739437	5.132058	-0.018270	2.127697
94.628694	1406.823377	5.137062	-0.018366	2.133115
94.916170	1414.905874	5.142067	-0.018425	2.138499
95.361139	1422.972965	5.147072	-0.018513	2.143873
95.920531	1431.058529	5.152077	-0.018622	2.149257
96.344647	1439.155353	5.157082	-0.018707	2.154622
96.434397	1447.273635	5.162086	-0.018729	2.159957
96.882204	1455.308354	5.167091	-0.018817	2.165257
97.417765	1463.391101	5.172096	-0.018922	2.170584
98.013117	1471.460676	5.177101	-0.019038	2.175894
98.313466	1479.536642	5.182106	-0.019099	2.181168
98.667894	1487.643071	5.187110	-0.019171	2.186454
98.905396	1495.770683	5.192115	-0.019220	2.191730
99.057085	1503.885346	5.197120	-0.019254	2.196977
99.365796	1511.945191	5.202125	-0.019316	2.202191
99.768056	1519.985894	5.207130	-0.019396	2.207389
100.070279	1528.099202	5.212134	-0.019458	2.212611
100.617982	1536.140969	5.217139	-0.019565	2.217798
100.882238	1544.220345	5.222144	-0.019620	2.222971
101.295036	1552.306078	5.227149	-0.019702	2.228149
101.566862	1560.402788	5.232154	-0.019758	2.233310
101.931759	1568.476316	5.237158	-0.019831	2.238452
102.493773	1576.512519	5.242163	-0.019941	2.243576
102.872069	1584.592319	5.247168	-0.020016	2.248699
103.093970	1592.732940	5.252173	-0.020063	2.253835
103.405560	1600.786169	5.257178	-0.020126	2.258913
103.993149	1608.824521	5.262182	-0.020241	2.263994
104.315354	1616.917311	5.267187	-0.020306	2.269074
104.699685	1625.078606	5.272192	-0.020383	2.274191
105.160353	1633.106730	5.277197	-0.020474	2.279220
105.270451	1641.174989	5.282202	-0.020500	2.284233
105.620981	1649.232798	5.287206	-0.020570	2.289249
105.787223	1657.358898	5.292211	-0.020607	2.294280
105.970978	1665.413813	5.297216	-0.020646	2.299258
106.477350	1673.456642	5.302221	-0.020745	2.304245
106.924313	1681.492770	5.307226	-0.020834	2.309211
107.020966	1689.626260	5.312230	-0.020857	2.314198
107.393074	1697.655130	5.317235	-0.020932	2.319132
107.707339	1705.716934	5.322240	-0.020995	2.324072
108.146506	1713.794813	5.327245	-0.021082	2.329020
108.375221	1721.873173	5.332250	-0.021130	2.333942
108.794176	1729.936517	5.337254	-0.021214	2.338859
109.137273	1737.996105	5.342259	-0.021283	2.343757
109.256372	1746.099182	5.347264	-0.021310	2.348654
109.576263	1754.202294	5.352269	-0.021375	2.353556
109.941242	1762.235527	5.357274	-0.021448	2.358409
110.345262	1770.275098	5.362278	-0.021529	2.363260
110.704877	1778.330902	5.367283	-0.021601	2.368106
111.277519	1786.363627	5.372288	-0.021713	2.372946
111.530737	1794.462494	5.377293	-0.021765	2.377790
111.484485	1802.545025	5.382298	-0.021762	2.382590
112.066423	1810.592341	5.387302	-0.021875	2.387410
112.241262	1818.685531	5.392307	-0.021913	2.392215
112.526052	1826.749533	5.397312	-0.021971	2.397001
112.936892	1834.797722	5.402317	-0.022053	2.401779
113.254365	1842.854167	5.407322	-0.022117	2.406544
113.627448	1850.926347	5.412326	-0.022192	2.411314
113.752640	1859.019586	5.417331	-0.022221	2.416067
114.267820	1867.036439	5.422336	-0.022322	2.420796
114.826342	1875.080459	5.427341	-0.022431	2.425535
115.132957	1883.166273	5.432346	-0.022493	2.430270
115.623055	1891.292830	5.437350	-0.022590	2.435033
116.099085	1899.295325	5.442355	-0.022684	2.439713
116.376020	1907.346906	5.447360	-0.022741	2.444398
116.804916	1915.403139	5.452365	-0.022826	2.449088
117.001807	1923.483241	5.457370	-0.022868	2.453766
117.504325	1931.519180	5.462374	-0.022966	2.458431
117.728146	1939.584770	5.467379	-0.023013	2.463084
117.869633	1947.663141	5.472384	-0.023045	2.467730
118.337834	1955.739739	5.477389	-0.023137	2.472390
118.535857	1963.799432	5.482394	-0.023179	2.477011
119.064824	1971.819919	5.487398	-0.023283	2.481626
119.142159	1979.903699	5.492403	-0.023303	2.486235
119.584784	1987.963037	5.497408	-0.023390	2.490848
119.758703	1996.060707	5.502413	-0.023428	2.495455
120.066600	2004.091361	5.507418	-0.023491	2.500025
120.627852	2012.116767	5.512422	-0.023600	2.504602
120.852216	2020.203249	5.517427	-0.023647	2.509180
120.903821	2028.329023	5.522432	-0.023662	2.513760
121.336308	2036.354469	5.527437	-0.023748	2.518303
121.553635	2044.378194	5.532442	-0.023794	2.522820
121.959924	2052.426082	5.537446	-0.023875	2.527357
122.136182	2060.499285	5.542451	-0.023913	2.531883
122.386607	2068.542623	5.547456	-0.023964	2.536390
122.632008	2076.613971	5.552461	-0.024015	2.540904
123.027401	2084.608887	5.557466	-0.024094	2.545378
123.346607	2092.686592	5.562470	-0.024159	2.549885
123.688478	2100.763524	5.567475	-0.024228	2.554384
124.068244	2108.791669	5.572480	-0.024304	2.558852
124.718601	2116.797433	5.577485	-0.024430	2.563318
124.956647	2124.855570	5.582490	-0.024480	2.567776
125.262657	2132.946017	5.587494	-0.024542	2.572249
125.457217	2141.029743	5.592499	-0.024583	2.576703
125.621667	2149.085768	5.597504	-0.024619	2.581132
125.937892	2157.135902	5.602509	-0.024683	2.585560
126.339051	2165.178570	5.607514	-0.024763	2.589983
126.824827	2173.424593	5.612518	-0.024859	2.594514
126.951891	2181.421006	5.617523	-0.024888	2.598878
127.051834	2189.419083	5.622528	-0.024912	2.603233
127.528583	2197.422153	5.627533	-0.025006	2.607609
127.654531	2205.475499	5.632538	-0.025034	2.611981
128.062118	2213.534161	5.637542	-0.025115	2.616367
128.433598	2221.542205	5.642547	-0.025190	2.620716
128.614258	2229.570212	5.647552	-0.025229	2.625056
128.900927	2237.632533	5.652557	-0.025287	2.629415
129.090122	2245.707308	5.657562	-0.025328	2.633766
129.339635	2253.756704	5.662566	-0.025379	2.638100
129.710464	2261.771087	5.667571	-0.025454	2.642417
129.894682	2269.818998	5.672576	-0.025493	2.646732
130.490399	2277.848059	5.677581	-0.025609	2.651057
130.851567	2285.901892	5.682586	-0.025682	2.655372
131.002269	2293.974699	5.687590	-0.025715	2.659677
131.375683	2302.006564	5.692595	-0.025790	2.663968
131.754495	2310.034454	5.697600	-0.025866	2.668250
132.098406	2318.142252	5.702605	-0.025935	2.672564
132.195514	2326.220507	5.707610	-0.025958	2.676841
132.788692	2334.207457	5.712614	-0.026074	2.681094
132.931197	2342.253463	5.717619	-0.026106	2.685343
133.108874	2350.302725	5.722624	-0.026144	2.689589
133.420660	2358.389753	5.727629	-0.026207	2.693856
133.500432	2366.436000	5.732634	-0.026227	2.698081
133.893356	2374.451448	5.737638	-0.026306	2.702302
134.052620	2382.521944	5.742643	-0.026341	2.706532
134.352724	2390.548249	5.747648	-0.026402	2.710740
134.809969	2398.611052	5.752653	-0.026492	2.714970
134.944097	2406.632669	5.757658	-0.026522	2.719152
135.119892	2414.681016	5.762662	-0.026560	2.723344
135.390631	2422.713754	5.767667	-0.026616	2.727528
135.858158	2430.750778	5.772672	-0.026708	2.731719
136.153066	2438.839550	5.777677	-0.026768	2.735920
136.329192	2446.860548	5.782682	-0.026806	2.740072
136.786934	2454.882473	5.787686	-0.026897	2.744236
136.990115	2462.950422	5.792691	-0.026940	2.748401
137.238030	2471.052232	5.797696	-0.026991	2.752580
137.533874	2479.124361	5.802701	-0.027052	2.756741
137.857992	2487.104949	5.807706	-0.027117	2.760850
138.078798	2495.148764	5.812710	-0.027163	2.764979
138.487331	2503.173064	5.817715	-0.027245	2.769102
138.836417	2511.235472	5.822720	-0.027315	2.773236
139.197461	2519.283577	5.827725	-0.027387	2.777357
139.261486	2527.326699	5.832730	-0.027405	2.781451
139.486130	2535.370500	5.837734	-0.027452	2.785549
139.756040	2543.400718	5.842739	-0.027507	2.789637
140.154966	2551.448964	5.847744	-0.027587	2.793736
140.515464	2559.480939	5.852749	-0.027659	2.797818
140.659320	2567.529968	5.857754	-0.027691	2.801890
141.094538	2575.531314	5.862758	-0.027777	2.805949
141.456598	2583.565915	5.867763	-0.027850	2.810014
141.580370	2591.664490	5.872768	-0.027878	2.814092
141.799892	2599.712290	5.877773	-0.027924	2.818144
142.056635	2607.739508	5.882778	-0.027977	2.822182
142.285005	2615.789095	5.887782	-0.028025	2.826224
142.680544	2623.839470	5.892787	-0.028104	2.830270
142.993963	2631.897762	5.897792	-0.028168	2.834309
143.165554	2639.953072	5.902797	-0.028205	2.838333
143.278897	2647.962463	5.907802	-0.028231	2.842325
143.565029	2655.987578	5.912806	-0.028290	2.846329
143.923091	2664.034313	5.917811	-0.028361	2.850342
144.045688	2672.090701	5.922816	-0.028389	2.854341
144.431021	2680.137809	5.927821	-0.028466	2.858345
144.904716	2688.122659	5.932826	-0.028560	2.862316
145.343080	2696.168407	5.937830	-0.028647	2.866311
145.311703	2704.256522	5.942835	-0.028646	2.870294
145.777124	2712.303663	5.947840	-0.028738	2.874280
146.041274	2720.325501	5.952845	-0.028792	2.878236
146.027501	2728.369025	5.957850	-0.028795	2.882182
146.336486	2736.391611	5.962854	-0.028858	2.886130
146.559930	2744.430358	5.967859	-0.028905	2.890076
146.762577	2752.482518	5.972864	-0.028948	2.894022
146.940813	2760.544637	5.977869	-0.028986	2.897966
147.162622	2768.563686	5.982874	-0.029033	2.901886
147.532118	2776.588390	5.987878	-0.029107	2.905811
147.784109	2784.626114	5.992883	-0.029159	2.909731
147.775494	2792.805055	5.997888	-0.029162	2.913700
147.987297	2800.816373	6.002893	-0.029207	2.917595
148.052192	2808.805495	6.007898	-0.029224	2.921465
148.415953	2816.806956	6.012902	-0.029297	2.925353
148.825123	2824.802678	6.017907	-0.029379	2.929234
148.677351	2832.904661	6.022912	-0.029356	2.933133
148.966192	2840.945402	6.027917	-0.029415	2.937019
149.153545	2848.962450	6.032922	-0.029455	2.940884
149.540159	2856.965393	6.037926	-0.029533	2.944747
149.625726	2865.006281	6.042931	-0.029554	2.948608
149.862454	2873.070857	6.047936	-0.029603	2.952483
150.367884	2881.105564	6.052941	-0.029702	2.956352
150.460054	2889.105100	6.057946	-0.029725	2.960178
150.868935	2897.130940	6.062950	-0.029806	2.964027
151.005599	2905.187973	6.067955	-0.029837	2.967873
151.229146	2913.234461	6.072960	-0.029884	2.971713
151.749582	2921.282261	6.077965	-0.029986	2.975564
151.934423	2929.290822	6.082970	-0.030025	2.979374
152.225987	2937.339296	6.087974	-0.030085	2.983203
152.404479	2945.391753	6.092979	-0.030123	2.987024
152.738638	2953.426295	6.097984	-0.030191	2.990839
152.983570	2961.508471	6.102989	-0.030242	2.994667
152.984713	2969.519441	6.107994	-0.030247	2.998445
153.188564	2977.549755	6.112998	-0.030290	3.002237
153.476865	2985.564884	6.118003	-0.030349	3.006021
153.699831	2993.583139	6.123008	-0.030396	3.009799
154.139059	3001.636293	6.128013	-0.030483	3.013599
154.244279	3009.657312	6.133018	-0.030508	3.017362
154.805366	3017.692402	6.138022	-0.030617	3.021150
154.740179	3025.736043	6.143027	-0.030611	3.024906
155.082111	3033.754171	6.148032	-0.030679	3.028666
155.620735	3041.807673	6.153037	-0.030785	3.032446
155.652841	3049.879511	6.158042	-0.030796	3.036207
155.897232	3057.887790	6.163046	-0.030847	3.039943
156.221215	3065.918049	6.168051	-0.030912	3.043688
156.475227	3073.950741	6.173056	-0.030965	3.047427
156.613307	3082.014749	6.178061	-0.030996	3.051170
156.801538	3090.061335	6.183066	-0.031036	3.054902
157.185774	3098.089084	6.188070	-0.031113	3.058631
157.135479	3106.136571	6.193075	-0.031109	3.062344
157.307097	3114.131956	6.198080	-0.031146	3.066038
157.770215	3122.152282	6.203085	-0.031237	3.069753
157.965132	3130.291224	6.208090	-0.031279	3.073506
158.124285	3138.318715	6.213094	-0.031314	3.077201
158.314022	3146.328351	6.218099	-0.031354	3.080885
158.610803	3154.282374	6.223104	-0.031415	3.084544
159.097422	3162.313602	6.228109	-0.031511	3.088243
159.075627	3170.373572	6.233114	-0.031512	3.091927
159.316273	3178.441518	6.238118	-0.031562	3.095622
159.681021	3186.434243	6.243123	-0.031635	3.099284
159.818903	3194.446196	6.248128	-0.031666	3.102940
160.162569	3202.496638	6.253133	-0.031735	3.106619
160.378592	3210.518613	6.258138	-0.031780	3.110275
160.861108	3218.558148	6.263142	-0.031876	3.113946
160.938870	3226.609551	6.268147	-0.031895	3.117600
161.040144	3234.639156	6.273152	-0.031919	3.121241
161.389275	3242.655166	6.278157	-0.031990	3.124882
161.482211	3250.694138	6.283162	-0.032012	3.128518
161.873281	3258.734040	6.288166	-0.032090	3.132164
162.078863	3266.793355	6.293171	-0.032134	3.135806
162.102161	3274.799476	6.298176	-0.032143	3.139411
162.645752	3282.844668	6.303181	-0.032250	3.143053
162.931846	3290.835513	6.308186	-0.032308	3.146655
163.094412	3298.898486	6.313190	-0.032344	3.150280
163.084329	3306.991748	6.318195	-0.032347	3.153906
163.462104	3314.982844	6.323200	-0.032422	3.157500
163.759304	3322.993114	6.328205	-0.032483	3.161094
163.953817	3330.955401	6.333210	-0.032524	3.164658
164.413575	3339.022414	6.338214	-0.032615	3.168277
164.765733	3347.075560	6.343219	-0.032686	3.171880
164.854211	3355.134514	6.348224	-0.032708	3.175471
165.120565	3363.170191	6.353229	-0.032763	3.179054
165.374101	3371.148063	6.358234	-0.032815	3.182608
165.472257	3379.218783	6.363238	-0.032838	3.186192
165.544774	3387.260894	6.368243	-0.032857	3.189758
166.051231	3395.286463	6.373248	-0.032957	3.193331
166.331507	3403.345492	6.378253	-0.033014	3.196906
166.288582	3411.345854	6.383258	-0.033011	3.200437
166.580521	3419.354666	6.388262	-0.033071	3.203981
167.010428	3427.380098	6.393267	-0.033156	3.207535
167.182275	3435.440977	6.398272	-0.033193	3.211090
167.428835	3443.484705	6.403277	-0.033245	3.214636
167.719541	3451.486374	6.408282	-0.033304	3.218162
168.022702	3459.541385	6.413286	-0.033366	3.221708
168.173321	3467.548318	6.418291	-0.033399	3.225222
168.099222	3475.600616	6.423296	-0.033390	3.228743
168.400459	3483.711235	6.428301	-0.033452	3.232301
168.504386	3491.712560	6.433306	-0.033476	3.235800
168.881089	3499.710344	6.438310	-0.033551	3.239304
169.079739	3507.721890	6.443315	-0.033594	3.242803
169.187935	3515.764851	6.448320	-0.033619	3.246309
169.347329	3523.760870	6.453325	-0.033654	3.249792
169.760267	3531.787685	6.458330	-0.033736	3.253295
169.869839	3539.860390	6.463334	-0.033762	3.256802
170.101156	3547.861588	6.468339	-0.033810	3.260279
170.418204	3555.870877	6.473344	-0.033874	3.263759
170.815550	3563.895324	6.478349	-0.033953	3.267245
170.990139	3571.921210	6.483354	-0.033991	3.270719
171.450926	3579.963918	6.488358	-0.034082	3.274208
171.563251	3588.013478	6.493363	-0.034108	3.277682
171.642852	3596.041214	6.498368	-0.034128	3.281142
171.981288	3604.025225	6.503373	-0.034197	3.284590
172.161593	3612.087182	6.508378	-0.034235	3.288061
172.393600	3620.126944	6.513382	-0.034284	3.291521
172.750774	3628.169241	6.518387	-0.034355	3.294984
173.119912	3636.157861	6.523392	-0.034429	3.298420
173.553601	3644.191614	6.528397	-0.034515	3.301874
173.741010	3652.200245	6.533402	-0.034555	3.305305
173.903047	3660.249524	6.538406	-0.034591	3.308748
174.104491	3668.316253	6.543411	-0.034634	3.312196
174.285512	3676.372030	6.548416	-0.034673	3.315636
174.461810	3684.351560	6.553421	-0.034711	3.319039
174.821158	3692.360089	6.558426	-0.034783	3.322458
175.090481	3700.370933	6.563430	-0.034838	3.325871
175.236113	3708.421523	6.568435	-0.034870	3.329293
175.405930	3716.463635	6.573440	-0.034907	3.332708
175.724828	3724.532142	6.578445	-0.034972	3.336137
175.946060	3732.517879	6.583450	-0.035018	3.339523
176.146497	3740.550585	6.588454	-0.035061	3.342925
176.269409	3748.587894	6.593459	-0.035089	3.346323
176.495935	3756.595652	6.598464	-0.035136	3.349708
176.810180	3764.661197	6.603469	-0.035200	3.353118
176.956923	3772.708613	6.608474	-0.035233	3.356510
177.137351	3780.701943	6.613478	-0.035271	3.359878
177.425054	3788.700949	6.618483	-0.035330	3.363248
177.753854	3796.702399	6.623488	-0.035397	3.366617
178.147434	3804.754975	6.628493	-0.035475	3.370007
178.176557	3812.810855	6.633498	-0.035486	3.373381
178.356950	3820.885213	6.638502	-0.035525	3.376766
178.596825	3828.877558	6.643507	-0.035574	3.380114
179.027931	3836.844692	6.648512	-0.035660	3.383456
179.193611	3844.927512	6.653517	-0.035696	3.386833
179.546598	3852.930874	6.658522	-0.035767	3.390180
179.813697	3861.041776	6.663526	-0.035822	3.393565
179.938536	3869.078847	6.668531	-0.035850	3.396912
180.360076	3877.021106	6.673536	-0.035934	3.400226
180.706847	3885.041478	6.678541	-0.036004	3.403566
180.920100	3893.072636	6.683546	-0.036049	3.406904
181.043263	3901.101852	6.688550	-0.036077	3.410233
181.274877	3909.156491	6.693555	-0.036125	3.413574
181.526736	3917.141918	6.698560	-0.036177	3.416884
181.752808	3925.197073	6.703565	-0.036225	3.420218
181.708377	3933.189904	6.708570	-0.036222	3.423514
182.130290	3941.219921	6.713574	-0.036305	3.426838
182.269715	3949.270252	6.718579	-0.036337	3.430158
182.424685	3957.291510	6.723584	-0.036371	3.433463
183.025133	3965.330951	6.728589	-0.036488	3.436787
183.437375	3973.294734	6.733594	-0.036570	3.440070
183.749825	3981.319276	6.738598	-0.036633	3.443372
183.947054	3989.377683	6.743603	-0.036675	3.446681
184.305515	3997.381443	6.748608	-0.036747	3.449969
184.498974	4005.480260	6.753613	-0.036788	3.453288
184.579277	4013.505771	6.758618	-0.036808	3.456570
184.931875	4021.504324	6.763622	-0.036879	3.459846
185.110143	4029.545884	6.768627	-0.036918	3.463132
185.249875	4037.560652	6.773632	-0.036949	3.466402
185.462931	4045.591860	6.778637	-0.036994	3.469678
185.604669	4053.654806	6.783642	-0.037025	3.472961
185.774476	4061.692503	6.788646	-0.037062	3.476232
185.966639	4069.663771	6.793651	-0.037103	3.479474
186.150171	4077.683295	6.798656	-0.037142	3.482731
186.419974	4085.706790	6.803661	-0.037198	3.485990
186.565766	4093.722859	6.808666	-0.037230	3.489239
186.986928	4101.750640	6.813670	-0.037314	3.492499
187.322719	4109.812821	6.818675	-0.037382	3.495766
187.454969	4117.798559	6.823680	-0.037411	3.498994
187.792642	4125.820878	6.828685	-0.037480	3.502239
188.070759	4133.830557	6.833690	-0.037537	3.505474
188.236882	4141.872631	6.838694	-0.037573	3.508716
188.366991	4149.942062	6.843699	-0.037602	3.511965
188.780086	4157.939196	6.848704	-0.037684	3.515190
189.107201	4165.954288	6.853709	-0.037750	3.518417
189.236543	4173.980956	6.858714	-0.037780	3.521640
189.339517	4181.962458	6.863718	-0.037804	3.524840
189.549638	4190.050112	6.868723	-0.037848	3.528084
189.702610	4198.066029	6.873728	-0.037882	3.531294
190.079344	4206.114778	6.878733	-0.037958	3.534521
190.147590	4214.168280	6.883738	-0.037975	3.537737
190.387643	4222.177191	6.888742	-0.038025	3.540938
190.773096	4230.145035	6.893747	-0.038102	3.544124
190.985140	4238.195854	6.898752	-0.038147	3.547335
191.099027	4246.251902	6.903757	-0.038173	3.550543
191.261555	4254.355730	6.908762	-0.038209	3.553767
191.563758	4262.377267	6.913766	-0.038270	3.556960
191.828602	4270.350621	6.918771	-0.038325	3.560130
191.761935	4278.330225	6.923776	-0.038318	3.563291
192.245621	4286.376161	6.928781	-0.038413	3.566490
192.226617	4294.361087	6.933786	-0.038415	3.569648
192.319678	4302.431891	6.938790	-0.038437	3.572840
192.550024	4310.470765	6.943795	-0.038485	3.576021
192.687840	4318.434115	6.948800	-0.038516	3.579166
193.113848	4326.499506	6.953805	-0.038601	3.582357
193.112742	4334.483164	6.958810	-0.038606	3.585501
193.480576	4342.499835	6.963814	-0.038679	3.588666
193.676245	4350.577358	6.968819	-0.038721	3.591846
193.996719	4358.569754	6.973824	-0.038786	3.594994
194.443423	4366.586620	6.978829	-0.038874	3.598152
194.562059	4374.584557	6.983834	-0.038902	3.601291
194.698002	4382.589109	6.988838	-0.038932	3.604430
194.706936	4390.649549	6.993843	-0.038939	3.607585
194.992810	4398.647300	6.998848	-0.038997	3.610720
195.366477	4406.722747	7.003853	-0.039072	3.613885
195.675577	4414.716334	7.008858	-0.039135	3.617014
195.866536	4422.732416	7.013862	-0.039176	3.620145
196.191371	4430.755062	7.018867	-0.039242	3.623280
196.524798	4438.770576	7.023872	-0.039309	3.626410
196.533314	4446.838071	7.028877	-0.039316	3.629548
196.826129	4454.884965	7.033882	-0.039375	3.632683
196.992775	4462.934735	7.038886	-0.039412	3.635813
197.171370	4470.916641	7.043891	-0.039450	3.638915
197.603381	4478.876074	7.048896	-0.039536	3.642011
197.745260	4486.921084	7.053901	-0.039567	3.645131
197.925862	4494.965588	7.058906	-0.039606	3.648248
198.103595	4503.014025	7.063910	-0.039645	3.651365
198.524827	4511.044117	7.068915	-0.039728	3.654478
198.700516	4519.051630	7.073920	-0.039766	3.657573
198.982327	4527.087247	7.078925	-0.039824	3.660679
199.178183	4535.081256	7.083930	-0.039865	3.663764
199.318071	4543.119090	7.088934	-0.039897	3.666862
199.424457	4551.170077	7.093939	-0.039922	3.669962
199.610972	4559.186860	7.098944	-0.039962	3.673047
199.979378	4567.242386	7.103949	-0.040036	3.676150
200.029766	4575.195579	7.108954	-0.040050	3.679203
200.376941	4583.227989	7.113958	-0.040120	3.682291
200.549112	4591.222494	7.118963	-0.040157	3.685357
200.596003	4599.220490	7.123968	-0.040171	3.688419
200.934318	4607.314019	7.128973	-0.040239	3.691522
201.188785	4615.310412	7.133978	-0.040292	3.694584
201.518403	4623.370062	7.138982	-0.040359	3.697669
201.721716	4631.374318	7.143987	-0.040402	3.700727
201.803966	4639.356194	7.148992	-0.040422	3.703771
202.147624	4647.416513	7.153997	-0.040491	3.706848
202.187419	4655.413623	7.159002	-0.040504	3.709892
202.397214	4663.523164	7.164006	-0.040548	3.712980
202.832839	4671.576709	7.169011	-0.040635	3.716050
202.975023	4679.515782	7.174016	-0.040666	3.719066
203.171254	4687.560090	7.179021	-0.040708	3.722121
203.390246	4695.508280	7.184026	-0.040754	3.725138
203.450833	4703.538122	7.189030	-0.040770	3.728179
203.630964	4711.571211	7.194035	-0.040809	3.731222
203.718578	4719.629931	7.199040	-0.040831	3.734271
204.195289	4727.643825	7.204045	-0.040925	3.737308
204.409182	4735.634378	7.209050	-0.040970	3.740328
204.359868	4743.667615	7.214054	-0.040966	3.743356
204.788578	4751.709439	7.219059	-0.041051	3.746396
204.676110	4759.709863	7.224064	-0.041035	3.749405
204.931253	4767.789696	7.229069	-0.041088	3.752450
205.158304	4775.827229	7.234074	-0.041135	3.755475
205.429754	4783.802949	7.239078	-0.041191	3.758477
205.706852	4791.856415	7.244083	-0.041248	3.761505
205.739215	4799.798808	7.249088	-0.041259	3.764483
206.005735	4807.876832	7.254093	-0.041314	3.767515
206.272064	4815.889740	7.259098	-0.041369	3.770520
206.751975	4823.913942	7.264102	-0.041463	3.773532
207.009036	4831.958881	7.269107	-0.041516	3.776544
207.192640	4839.950317	7.274112	-0.041556	3.779532
207.505360	4847.979870	7.279117	-0.041619	3.782535
207.739147	4856.001334	7.284122	-0.041668	3.785531
208.050935	4864.012940	7.289126	-0.041731	3.788522
207.998793	4872.101843	7.294131	-0.041727	3.791531
208.166752	4880.117129	7.299136	-0.041763	3.794516
208.587311	4888.122430	7.304141	-0.041847	3.797500
208.793909	4896.108774	7.309146	-0.041890	3.800470
208.816695	4904.100299	7.314150	-0.041900	3.803436
209.302164	4912.160733	7.319155	-0.041995	3.806434
209.518639	4920.113342	7.324160	-0.042041	3.809385
209.746791	4928.225116	7.329165	-0.042089	3.812392
209.764541	4936.229574	7.334170	-0.042097	3.815353
209.850034	4944.243177	7.339174	-0.042118	3.818317
210.218487	4952.258875	7.344179	-0.042192	3.821284
210.250825	4960.264381	7.349184	-0.042203	3.824239
210.578001	4968.288328	7.354189	-0.042270	3.827204
210.737503	4976.298369	7.359194	-0.042304	3.830159
210.808487	4984.344216	7.364198	-0.042323	3.833122
211.056464	4992.390728	7.369203	-0.042374	3.836087
211.275415	5000.361917	7.374208	-0.042420	3.839022
211.596859	5008.406779	7.379213	-0.042485	3.841983
211.716330	5016.375497	7.384218	-0.042513	3.844910
212.029146	5024.400212	7.389222	-0.042576	3.847859
212.296320	5032.482305	7.394227	-0.042631	3.850825
212.469118	5040.470120	7.399232	-0.042669	3.853754
212.577181	5048.546993	7.404237	-0.042694	3.856711
212.775233	5056.531282	7.409242	-0.042736	3.859634
212.822281	5064.544382	7.414246	-0.042750	3.862562
213.142433	5072.584017	7.419251	-0.042815	3.865503
213.430630	5080.587959	7.424256	-0.042874	3.868428
213.625736	5088.650181	7.429261	-0.042915	3.871370
213.694893	5096.914839	7.434266	-0.042933	3.874381
213.820831	5104.836228	7.439270	-0.042962	3.877266
214.129022	5112.737659	7.444275	-0.043025	3.880145
214.281826	5120.745223	7.449280	-0.043058	3.883058
214.649098	5128.757981	7.454285	-0.043132	3.885974
214.820065	5136.748411	7.459290	-0.043169	3.888876
214.920088	5144.820936	7.464294	-0.043193	3.891805
214.889736	5152.874432	7.469299	-0.043192	3.894721
215.133813	5160.837865	7.474304	-0.043243	3.897609
215.661166	5168.817822	7.479309	-0.043346	3.900505
215.851487	5176.840177	7.484314	-0.043387	3.903408
216.090758	5184.881667	7.489318	-0.043437	3.906317
216.418493	5192.917853	7.494323	-0.043503	3.909223
216.292916	5200.962279	7.499328	-0.043485	3.912122
216.505048	5208.987833	7.504333	-0.043529	3.915018
216.612890	5216.982158	7.509338	-0.043555	3.917899
216.618425	5224.977110	7.514342	-0.043561	3.920776
216.785584	5232.977726	7.519347	-0.043597	3.923655
217.250068	5241.000864	7.524352	-0.043689	3.926546
217.374613	5249.020795	7.529357	-0.043717	3.929428
217.386400	5257.063531	7.534362	-0.043725	3.932314
217.538391	5265.071351	7.539366	-0.043758	3.935187
218.136959	5273.116509	7.544371	-0.043875	3.938080
218.276770	5281.086294	7.549376	-0.043906	3.940935
218.400094	5289.110744	7.554381	-0.043934	3.943807
218.656507	5297.142559	7.559386	-0.043987	3.946683
218.613010	5305.164128	7.564390	-0.043984	3.949547
218.672691	5313.235583	7.569395	-0.044001	3.952429
218.968859	5321.226406	7.574400	-0.044061	3.955284
219.414559	5329.249354	7.579405	-0.044149	3.958151
219.441933	5337.232278	7.584410	-0.044160	3.960995
219.759112	5345.208222	7.589414	-0.044224	3.963839
219.833384	5353.287462	7.594419	-0.044243	3.966713
219.908884	5361.255659	7.599424	-0.044262	3.969546
220.115241	5369.336969	7.604429	-0.044306	3.972419
220.241026	5377.346977	7.609434	-0.044335	3.975264
220.447232	5385.367010	7.614438	-0.044378	3.978111
220.747704	5393.363008	7.619443	-0.044439	3.980949
220.822991	5401.361884	7.624448	-0.044458	3.983783
221.191415	5409.427328	7.629453	-0.044532	3.986642
221.370746	5417.423364	7.634458	-0.044571	3.989472
221.700766	5425.480253	7.639462	-0.044638	3.992324
221.877565	5433.526034	7.644467	-0.044676	3.995168
221.918866	5441.527022	7.649472	-0.044689	3.997991
222.101148	5449.555776	7.654477	-0.044728	4.000825
222.368801	5457.542208	7.659482	-0.044783	4.003643
222.556339	5465.566301	7.664486	-0.044823	4.006471
222.688759	5473.581699	7.669491	-0.044853	4.009293
222.872357	5481.623672	7.674496	-0.044892	4.012123
222.966440	5489.709078	7.679501	-0.044915	4.014965
223.237399	5497.724112	7.684506	-0.044971	4.017783
223.301320	5505.699502	7.689510	-0.044988	4.020582
223.688482	5513.703159	7.694515	-0.045065	4.023393
223.835487	5521.705890	7.699520	-0.045098	4.026199
223.963463	5529.756118	7.704525	-0.045127	4.029019
224.362749	5537.761302	7.709530	-0.045206	4.031825
224.640856	5545.874715	7.714534	-0.045263	4.034666
224.812056	5553.888482	7.719539	-0.045300	4.037468
224.800510	5561.800999	7.724544	-0.045303	4.040230
225.890230	5569.790538	7.729549	-0.045511	4.043033
226.211006	5577.808868	7.734554	-0.045576	4.045833
226.573040	5585.806097	7.739558	-0.045649	4.048624
226.744594	5593.898432	7.744563	-0.045686	4.051443
226.845061	5601.911394	7.749568	-0.045710	4.054232
227.132734	5609.934023	7.754573	-0.045769	4.057025
227.383798	5617.907145	7.759578	-0.045821	4.059798
227.444491	5625.943844	7.764582	-0.045837	4.062589
227.811334	5633.959484	7.769587	-0.045911	4.065375
227.838683	5641.964531	7.774592	-0.045921	4.068150
228.192414	5650.013557	7.779597	-0.045992	4.070944
228.249390	5658.042042	7.784602	-0.046008	4.073724
228.389528	5666.068277	7.789606	-0.046039	4.076502
228.749127	5674.072543	7.794611	-0.046111	4.079274
228.899486	5682.075145	7.799616	-0.046145	4.082041
229.157513	5690.064626	7.804621	-0.046198	4.084803
229.172048	5698.130515	7.809626	-0.046206	4.087586
229.316279	5706.139902	7.814630	-0.046238	4.090349
229.530290	5714.190197	7.819635	-0.046283	4.093125
229.793929	5722.170709	7.824640	-0.046337	4.095876
229.981354	5730.182257	7.829645	-0.046377	4.098635
229.986187	5738.220640	7.834650	-0.046384	4.101399
230.284139	5746.188125	7.839654	-0.046444	4.104141
230.582623	5754.265646	7.844659	-0.046505	4.106918
230.663783	5762.255726	7.849664	-0.046525	4.109661
230.946886	5770.364025	7.854669	-0.046583	4.112445
230.961476	5778.369225	7.859674	-0.046591	4.115188
231.006578	5786.369558	7.864678	-0.046605	4.117928
231.313264	5794.356711	7.869683	-0.046667	4.120665
231.441663	5802.375777	7.874688	-0.046696	4.123409
231.621542	5810.380138	7.879693	-0.046735	4.126147
231.809274	5818.423454	7.884698	-0.046775	4.128896
231.872988	5826.465599	7.889702	-0.046792	4.131642
232.102741	5834.509150	7.894707	-0.046840	4.134388
232.374567	5842.486135	7.899712	-0.046896	4.137110
232.394231	5850.501054	7.904717	-0.046905	4.139840
232.663153	5858.521883	7.909722	-0.046960	4.142573
232.858729	5866.487286	7.914726	-0.047002	4.145285
232.979274	5874.594678	7.919731	-0.047029	4.148042
233.197526	5882.563561	7.924736	-0.047075	4.150752
233.574226	5890.637297	7.929741	-0.047151	4.153497
233.529086	5898.679081	7.934746	-0.047147	4.156225
233.856600	5906.636383	7.939750	-0.047214	4.158926
234.054830	5914.666871	7.944755	-0.047256	4.161649
234.284883	5922.632486	7.949760	-0.047304	4.164349
234.324271	5930.700967	7.954765	-0.047316	4.167079
234.442578	5938.706630	7.959770	-0.047344	4.169788
234.627903	5946.711698	7.964774	-0.047383	4.172495
234.944242	5954.777963	7.969779	-0.047447	4.175222
235.214771	5962.758559	7.974784	-0.047503	4.177918
235.495377	5970.786707	7.979789	-0.047560	4.180629
235.435743	5978.785483	7.984794	-0.047554	4.183324
235.486029	5986.786893	7.989798	-0.047569	4.186020
235.671804	5994.857940	7.994803	-0.047609	4.188738
235.904351	6002.859525	7.999808	-0.047657	4.191432
236.042014	6010.971465	8.004813	-0.047688	4.194161
235.984491	6019.025904	8.009818	-0.047683	4.196866
236.184833	6026.879579	8.014822	-0.047725	4.199505
236.417360	6034.931857	8.019827	-0.047774	4.202208
236.588735	6042.850606	8.024832	-0.047811	4.204865
236.880979	6050.899471	8.029837	-0.047870	4.207565
236.896872	6058.951524	8.034842	-0.047879	4.210262
236.901503	6066.965221	8.039846	-0.047885	4.212943
237.221482	6075.016882	8.044851	-0.047950	4.215639
237.304054	6083.007810	8.049856	-0.047970	4.218311
237.540022	6091.020014	8.054861	-0.048019	4.220989
237.600913	6099.015268	8.059866	-0.048036	4.223659
238.102129	6107.030299	8.064870	-0.048134	4.226337
238.325321	6115.114653	8.069875	-0.048181	4.229034
238.205644	6123.105096	8.074880	-0.048164	4.231695
238.460415	6131.134235	8.079885	-0.048217	4.234370
238.722056	6139.161805	8.084890	-0.048271	4.237044
239.021864	6147.123076	8.089894	-0.048332	4.239694
239.091587	6155.154908	8.094899	-0.048350	4.242363
239.024996	6163.120274	8.099904	-0.048343	4.245008
239.395501	6171.204993	8.104909	-0.048417	4.247694
239.694605	6179.187662	8.109914	-0.048478	4.250345
239.937760	6187.279615	8.114918	-0.048528	4.253029
240.151681	6195.333241	8.119923	-0.048573	4.255699
240.387584	6203.318808	8.124928	-0.048622	4.258344
240.380589	6211.345907	8.129933	-0.048626	4.261000
240.509611	6219.344317	8.134938	-0.048656	4.263645
240.759410	6227.334295	8.139942	-0.048707	4.266288
240.967518	6235.387129	8.144947	-0.048751	4.268948
241.075288	6243.394591	8.149952	-0.048776	4.271592
241.563906	6251.453501	8.154957	-0.048873	4.274254
241.682351	6259.502101	8.159962	-0.048900	4.276907
241.794972	6267.426005	8.164966	-0.048926	4.279518
242.081978	6275.511865	8.169971	-0.048985	4.282182
242.158114	6283.418083	8.174976	-0.049004	4.284784
242.317969	6291.521877	8.179981	-0.049039	4.287449
242.421267	6299.481946	8.184986	-0.049064	4.290066
242.604312	6307.562039	8.189990	-0.049103	4.292720
242.894070	6315.602868	8.194995	-0.049162	4.295361
243.084941	6323.565344	8.200000	-0.049203	4.297974
243.374213	6331.580052	8.205005	-0.049262	4.300603
243.504801	6339.617679	8.210010	-0.049291	4.303237
243.779345	6347.611272	8.215014	-0.049348	4.305856
244.221413	6355.653860	8.220019	-0.049435	4.308490
244.198843	6363.624864	8.225024	-0.049436	4.311096
244.365688	6371.715072	8.230029	-0.049473	4.313740
244.699679	6379.692900	8.235034	-0.049540	4.316348
244.725270	6387.668905	8.240038	-0.049550	4.318951
244.756303	6395.736758	8.245043	-0.049561	4.321583
244.738805	6403.695598	8.250048	-0.049563	4.324177
245.270308	6411.755150	8.255053	-0.049667	4.326806
245.088903	6419.761637	8.260058	-0.049638	4.329411
245.142392	6427.791116	8.265062	-0.049654	4.332024
245.528723	6435.860031	8.270067	-0.049731	4.334650
245.514512	6443.852659	8.275072	-0.049733	4.337247
245.717264	6451.826541	8.280077	-0.049776	4.339838
246.061659	6459.870807	8.285082	-0.049846	4.342451
246.091627	6467.838573	8.290086	-0.049856	4.345036
246.358357	6475.894207	8.295091	-0.049911	4.347649
246.504457	6483.923365	8.300096	-0.049944	4.350251
246.830968	6491.980035	8.305101	-0.050010	4.352862
246.826842	6500.055576	8.310106	-0.050014	4.355475
246.992129	6507.969644	8.315110	-0.050050	4.358035
247.426593	6515.961784	8.320115	-0.050136	4.360621
247.540306	6523.940481	8.325120	-0.050163	4.363199
247.597897	6531.957845	8.330125	-0.050178	4.365787
247.802893	6540.001590	8.335130	-0.050222	4.368384
248.207530	6547.997320	8.340134	-0.050302	4.370964
248.348101	6556.086831	8.345139	-0.050334	4.373571
248.471526	6564.082614	8.350144	-0.050362	4.376147
248.848635	6572.046856	8.355149	-0.050437	4.378712
248.835960	6580.109820	8.360154	-0.050440	4.381306
249.059061	6588.062925	8.365158	-0.050487	4.383864
249.553511	6596.139792	8.370163	-0.050584	4.386461
249.633272	6604.110652	8.375168	-0.050604	4.389021
249.807936	6612.167415	8.380173	-0.050642	4.391607
250.104641	6620.214427	8.385178	-0.050703	4.394189
250.200107	6628.248963	8.390182	-0.050726	4.396765
250.324474	6636.222494	8.395187	-0.050754	4.399320
250.370198	6644.239951	8.400192	-0.050768	4.401887
250.604506	6652.217326	8.405197	-0.050816	4.404440
250.631174	6660.274764	8.410202	-0.050827	4.407017
250.609935	6668.254571	8.415206	-0.050828	4.409567
250.977553	6676.370304	8.420211	-0.050902	4.412161
251.060147	6684.377599	8.425216	-0.050922	4.414717
251.282895	6692.386642	8.430221	-0.050969	4.417273
251.521142	6700.331641	8.435226	-0.051018	4.419807
251.706656	6708.417268	8.440230	-0.051058	4.422384
251.990422	6716.403413	8.445235	-0.051116	4.424929
251.930947	6724.446876	8.450240	-0.051110	4.427488
252.030151	6732.438921	8.455245	-0.051134	4.430031
252.493255	6740.541960	8.460250	-0.051225	4.432609
252.697686	6748.522435	8.465254	-0.051269	4.435145
252.836512	6756.533951	8.470259	-0.051300	4.437690
252.896503	6764.487124	8.475264	-0.051316	4.440214
252.877719	6772.559031	8.480269	-0.051318	4.442774
253.233732	6780.524771	8.485274	-0.051389	4.445300
253.573643	6788.532839	8.490278	-0.051458	4.447838
253.642537	6796.569427	8.495283	-0.051476	4.450383
253.576274	6804.606244	8.500288	-0.051469	4.452926
253.939451	6812.635996	8.505293	-0.051542	4.455467
254.121759	6820.649715	8.510298	-0.051581	4.458000
254.385744	6828.613820	8.515302	-0.051635	4.460517
254.649802	6836.646831	8.520307	-0.051689	4.463054
254.711183	6844.651958	8.525312	-0.051706	4.465580
254.816953	6852.706758	8.530317	-0.051731	4.468120
255.092895	6860.705066	8.535322	-0.051788	4.470642
255.266925	6868.763520	8.540326	-0.051825	4.473181
255.525336	6876.778215	8.545331	-0.051879	4.475704
255.569333	6884.720121	8.550336	-0.051892	4.478203
255.728406	6892.762773	8.555341	-0.051927	4.480733
255.910292	6900.770092	8.560346	-0.051966	4.483250
256.000244	6908.770854	8.565351	-0.051988	4.485763
256.195696	6916.809078	8.570355	-0.052029	4.488287
256.141413	6924.821128	8.575360	-0.052024	4.490800
256.521748	6932.859046	8.580365	-0.052101	4.493322
256.646238	6940.894683	8.585370	-0.052129	4.495840
256.811557	6948.874745	8.590375	-0.052165	4.498340
257.122491	6956.898136	8.595379	-0.052228	4.500852
257.123376	6964.904440	8.600384	-0.052233	4.503357
257.467493	6972.915776	8.605389	-0.052303	4.505863
257.535812	6980.944606	8.610394	-0.052321	4.508372
257.714255	6988.947212	8.615399	-0.052359	4.510872
257.956421	6997.044962	8.620403	-0.052409	4.513400
258.255753	7005.029879	8.625408	-0.052470	4.515891
258.455534	7012.998906	8.630413	-0.052513	4.518377
258.432431	7021.024830	8.635418	-0.052514	4.520878
258.748709	7028.996108	8.640423	-0.052578	4.523361
259.134925	7037.067826	8.645427	-0.052655	4.525874
259.358195	7045.032630	8.650432	-0.052702	4.528352
259.425419	7053.059940	8.655437	-0.052719	4.530848
259.391056	7061.099244	8.660442	-0.052718	4.533347
259.489145	7069.103139	8.665447	-0.052742	4.535833
259.788783	7077.142752	8.670451	-0.052803	4.538329
259.945906	7085.114053	8.675456	-0.052837	4.540802
260.079821	7093.181516	8.680461	-0.052867	4.543304
260.126789	7101.165151	8.685466	-0.052881	4.545778
260.481458	7109.178225	8.690471	-0.052952	4.548260
260.697865	7117.195306	8.695475	-0.052998	4.550742
260.727278	7125.224548	8.700480	-0.053009	4.553226
260.951234	7133.277780	8.705485	-0.053055	4.555717
261.080116	7141.286282	8.710490	-0.053085	4.558192
261.117809	7149.254962	8.715495	-0.053097	4.560653
261.361050	7157.307358	8.720499	-0.053147	4.563139
261.514990	7165.245027	8.725504	-0.053181	4.565588
261.850254	7173.308157	8.730509	-0.053249	4.568075
261.593289	7181.338483	8.735514	-0.053206	4.570550
261.681817	7189.379553	8.740519	-0.053228	4.573027
262.229111	7197.418215	8.745523	-0.053335	4.575502
262.168029	7205.426772	8.750528	-0.053329	4.577966
262.295981	7213.386600	8.755533	-0.053358	4.580414
262.277199	7221.472809	8.760538	-0.053360	4.582900
262.574594	7229.419824	8.765543	-0.053420	4.585341
262.686594	7237.453694	8.770547	-0.053446	4.587808
263.111781	7245.498939	8.775552	-0.053531	4.590277
263.396926	7253.570101	8.780557	-0.053589	4.592752
263.431673	7261.594801	8.785562	-0.053601	4.595212
263.526527	7269.564713	8.790567	-0.053624	4.597654
263.743400	7277.553233	8.795571	-0.053669	4.600100
263.955237	7285.551195	8.800576	-0.053714	4.602547
264.133506	7293.558585	8.805581	-0.053752	4.604996
264.177100	7301.630453	8.810586	-0.053766	4.607464
264.319985	7309.567790	8.815591	-0.053797	4.609889
264.525689	7317.663869	8.820595	-0.053841	4.612362
264.883008	7325.645933	8.825600	-0.053913	4.614798
265.076188	7333.682233	8.830605	-0.053954	4.617249
265.116302	7341.618115	8.835610	-0.053966	4.619669
265.424571	7349.646890	8.840615	-0.054029	4.622115
265.723937	7357.659520	8.845619	-0.054090	4.624555
265.537673	7365.729641	8.850624	-0.054060	4.627012
265.878059	7373.736661	8.855629	-0.054129	4.629448
265.979417	7381.764794	8.860634	-0.054153	4.631889
266.348336	7389.755921	8.865639	-0.054227	4.634317
266.509174	7397.818551	8.870643	-0.054262	4.636766
266.814096	7405.778017	8.875648	-0.054324	4.639182
267.116864	7413.829231	8.880653	-0.054386	4.641625
267.057377	7421.793804	8.885658	-0.054380	4.644040
267.147596	7429.852758	8.890663	-0.054402	4.646483
267.568157	7437.827743	8.895667	-0.054485	4.648898
267.371571	7445.822825	8.900672	-0.054454	4.651320
267.469364	7453.844028	8.905677	-0.054477	4.653747
267.757539	7461.925118	8.910682	-0.054536	4.656191
267.892841	7469.903398	8.915687	-0.054567	4.658603
267.980187	7477.960031	8.920691	-0.054588	4.661037
268.161687	7485.920098	8.925696	-0.054627	4.663440
268.424729	7493.936545	8.930701	-0.054681	4.665860
268.570345	7501.991765	8.935706	-0.054714	4.668289
268.716465	7509.970467	8.940711	-0.054746	4.670695
269.110161	7518.120699	8.945715	-0.054825	4.673150
269.306420	7526.108216	8.950720	-0.054866	4.675556
269.318364	7534.075878	8.955725	-0.054874	4.677955
269.390609	7542.008619	8.960730	-0.054892	4.680341
269.600489	7550.026373	8.965735	-0.054937	4.682752
269.806375	7558.062864	8.970739	-0.054980	4.685167
269.813667	7566.057411	8.975744	-0.054987	4.687569
270.016025	7574.038842	8.980749	-0.055030	4.689965
270.246328	7582.172418	8.985754	-0.055078	4.692406
270.179441	7590.140319	8.990759	-0.055071	4.694796
270.505530	7598.205082	8.995763	-0.055137	4.697213
270.530875	7606.146536	9.000768	-0.055146	4.699593
270.788056	7614.198304	9.005773	-0.055200	4.702003
270.896278	7622.091296	9.010778	-0.055225	4.704366
271.203987	7630.145626	9.015783	-0.055287	4.706775
271.440498	7638.242192	9.020787	-0.055337	4.709195
271.470317	7646.200022	9.025792	-0.055347	4.711574
271.808068	7654.278801	9.030797	-0.055416	4.713986
272.079495	7662.317278	9.035802	-0.055471	4.716385
272.122511	7670.262446	9.040807	-0.055484	4.718756
272.257634	7678.366482	9.045811	-0.055515	4.721173
272.197876	7686.333381	9.050816	-0.055509	4.723548
272.409613	7694.299818	9.055821	-0.055554	4.725921
272.510958	7702.406521	9.060826	-0.055578	4.728335
272.854203	7710.330184	9.065831	-0.055647	4.730692
273.037328	7718.432489	9.070835	-0.055686	4.733102
272.986662	7726.451272	9.075840	-0.055682	4.735487
273.148642	7734.419811	9.080845	-0.055717	4.737855
273.432637	7742.460074	9.085850	-0.055775	4.740242
273.495153	7750.477663	9.090855	-0.055792	4.742622
273.660531	7758.433215	9.095859	-0.055828	4.744982
273.873995	7766.490258	9.100864	-0.055873	4.747371
274.124199	7774.499243	9.105869	-0.055925	4.749745
274.142094	7782.548366	9.110874	-0.055933	4.752130
274.583632	7790.562755	9.115879	-0.056021	4.754501
274.791956	7798.561373	9.120883	-0.056065	4.756868
274.737213	7806.577438	9.125888	-0.056060	4.759240
274.810705	7814.580217	9.130893	-0.056079	4.761606
274.977872	7822.578792	9.135898	-0.056115	4.763969
275.095256	7830.571203	9.140903	-0.056142	4.766330
275.417526	7838.596969	9.145907	-0.056207	4.768698
275.494301	7846.627568	9.150912	-0.056227	4.771068
275.645164	7854.635748	9.155917	-0.056260	4.773429
275.840763	7862.692048	9.160922	-0.056302	4.775804
275.946220	7870.671613	9.165927	-0.056327	4.778155
276.102853	7878.707883	9.170931	-0.056361	4.780521
276.031086	7886.670447	9.175936	-0.056353	4.782865
276.483328	7894.620619	9.180941	-0.056442	4.785202
276.778525	7902.753971	9.185946	-0.056502	4.787593
276.715630	7910.726450	9.190951	-0.056496	4.789936
276.905573	7918.827003	9.195955	-0.056537	4.792315
277.218365	7926.783717	9.200960	-0.056600	4.794650
277.292352	7934.824552	9.205965	-0.056619	4.797010
277.292596	7942.789376	9.210970	-0.056624	4.799346
277.630275	7950.821304	9.215975	-0.056692	4.801700
277.889143	7958.765389	9.220979	-0.056746	4.804027
277.979265	7966.852305	9.225984	-0.056768	4.806395
278.032072	7974.851937	9.230989	-0.056783	4.808737
278.359923	7982.907315	9.235994	-0.056849	4.811092
278.438592	7990.403937	9.240999	-0.056868	4.813285
278.558240	7995.107564	9.246003	-0.056894	4.814659

278.734021	7997.628075	9.251008	-0.056928	4.815395
278.895238	7998.725840	9.256013	-0.056959	4.815715
278.966319	7999.700274	9.261018	-0.056973	4.816000
278.987908	7999.657933	9.266023	-0.056977	4.815987
279.152021	7999.711109	9.271027	-0.057007	4.816002
279.111220	7999.739212	9.276032	-0.057000	4.816010
279.181741	7999.960551	9.281037	-0.057013	4.816074
279.380774	8000.036796	9.286042	-0.057050	4.816096
279.282580	7999.980534	9.291047	-0.057032	4.816080
279.369671	7999.988519	9.296051	-0.057048	4.816082
279.465004	8000.029771	9.301056	-0.057066	4.816093
279.475795	7999.883610	9.306061	-0.057068	4.816050
279.353560	8000.019203	9.311066	-0.057045	4.816091
279.455168	8000.220812	9.316071	-0.057064	4.816149
279.512137	8000.017798	9.321075	-0.057074	4.816089
279.558013	8000.131867	9.326080	-0.057083	4.816123
279.515529	8000.244335	9.331085	-0.057075	4.816156
279.615081	8000.030341	9.336090	-0.057093	4.816093
279.719601	8000.141199	9.341095	-0.057113	4.816124
279.803874	8000.026279	9.346099	-0.057129	4.816090
279.814071	8000.012574	9.351104	-0.057130	4.816086
280.029788	8000.090193	9.356109	-0.057171	4.816108
280.142290	8000.061248	9.361114	-0.057192	4.816099
280.120953	8000.239268	9.366119	-0.057188	4.816151
280.300911	8000.032069	9.371123	-0.057221	4.816089
280.098077	8000.141634	9.376128	-0.057183	4.816123
280.054405	8000.016918	9.381133	-0.057175	4.816086
280.336755	7999.994255	9.386138	-0.057228	4.816078
280.207244	7999.970541	9.391143	-0.057204	4.816072
280.156826	7999.977104	9.396147	-0.057194	4.816074
280.161368	8000.029532	9.401152	-0.057195	4.816089
280.229900	7999.950649	9.406157	-0.057208	4.816066
280.230951	8000.057497	9.411162	-0.057208	4.816097
280.157482	7999.965359	9.416167	-0.057194	4.816071
280.298082	8000.007431	9.421171	-0.057220	4.816082
280.272195	8000.093494	9.426176	-0.057216	4.816108
280.375310	7999.976778	9.431181	-0.057235	4.816073
280.361938	8000.035291	9.436186	-0.057232	4.816090
280.427844	8000.182843	9.441191	-0.057245	4.816133
280.572511	8000.140593	9.446195	-0.057271	4.816120
280.750089	8000.014542	9.451200	-0.057304	4.816082
280.688739	8000.052957	9.456205	-0.057293	4.816094
280.594223	7999.963641	9.461210	-0.057275	4.816068
280.665133	8000.088849	9.466215	-0.057289	4.816104
280.876864	7999.950597	9.471219	-0.057328	4.816063
280.652844	8000.124946	9.476224	-0.057286	4.816115
280.549863	7999.976719	9.481229	-0.057267	4.816072
280.798445	8000.043183	9.486234	-0.057313	4.816090
280.853618	7999.964057	9.491239	-0.057324	4.816067
281.004048	7999.899477	9.496243	-0.057352	4.816047
280.856994	7999.970525	9.501248	-0.057324	4.816069
280.770543	7999.927293	9.506253	-0.057308	4.816056
280.995336	7999.927091	9.511258	-0.057350	4.816055
280.890383	7999.990355	9.516263	-0.057330	4.816074
281.243823	7999.911292	9.521267	-0.057396	4.816049
281.171048	8000.062743	9.526272	-0.057383	4.816094
281.086898	7999.833663	9.531277	-0.057367	4.816027
281.092376	8000.000419	9.536282	-0.057368	4.816076
281.129349	8000.001087	9.541287	-0.057375	4.816076
280.974622	7999.906406	9.546291	-0.057346	4.816049
280.913193	7999.907429	9.551296	-0.057334	4.816050
281.152937	7999.954504	9.556301	-0.057379	4.816062
281.115103	7999.905742	9.561306	-0.057372	4.816048
281.040434	7999.999468	9.566311	-0.057358	4.816076
281.077594	7999.879419	9.571315	-0.057365	4.816041
280.997948	8000.017925	9.576320	-0.057350	4.816082
281.059366	8000.032924	9.581325	-0.057362	4.816086
281.338276	7999.892684	9.586330	-0.057413	4.816043
281.246621	8000.071570	9.591335	-0.057396	4.816096
281.272251	7999.974814	9.596339	-0.057401	4.816068
281.214111	8000.031449	9.601344	-0.057390	4.816084
281.157371	7999.838121	9.606349	-0.057380	4.816028
281.342756	7999.973950	9.611354	-0.057414	4.816067
281.384984	7999.888179	9.616359	-0.057422	4.816042
281.367921	7999.885732	9.621363	-0.057419	4.816041
281.351337	7999.955940	9.626368	-0.057416	4.816062
281.340075	7999.980305	9.631373	-0.057414	4.816069
281.297967	7999.880186	9.636378	-0.057406	4.816040
281.262316	7999.971415	9.641383	-0.057399	4.816067
281.495188	7999.855980	9.646387	-0.057442	4.816032
281.418479	8000.015907	9.651392	-0.057428	4.816079
281.420330	7999.909105	9.656397	-0.057428	4.816048
281.603926	7999.972258	9.661402	-0.057463	4.816065
281.464918	8000.012470	9.666407	-0.057437	4.816078
281.579583	7999.956856	9.671411	-0.057458	4.816061
281.744579	8000.027151	9.676416	-0.057489	4.816080
281.579655	8000.054073	9.681421	-0.057458	4.816089
281.618896	7999.915899	9.686426	-0.057465	4.816049
281.562650	8000.075129	9.691431	-0.057455	4.816095
281.649258	7999.847004	9.696435	-0.057471	4.816028
281.606755	8000.032123	9.701440	-0.057463	4.816083
281.426962	8000.048093	9.706445	-0.057430	4.816088
281.613690	7999.905113	9.711450	-0.057464	4.816045
281.487578	8000.115425	9.716455	-0.057441	4.816108
281.518496	7999.862789	9.721459	-0.057447	4.816034
281.568272	8000.000436	9.726464	-0.057456	4.816074
281.421490	7999.799065	9.731469	-0.057428	4.816015
281.315771	8000.014018	9.736474	-0.057409	4.816079
281.278050	8000.052861	9.741479	-0.057402	4.816090
281.644424	7999.983648	9.746483	-0.057470	4.816068
281.569661	8000.029298	9.751488	-0.057456	4.816082
281.625851	7999.936301	9.756493	-0.057466	4.816054
281.779032	7999.924119	9.761498	-0.057495	4.816050
281.566647	7999.925610	9.766503	-0.057455	4.816052
281.580137	7999.973928	9.771507	-0.057458	4.816066
281.826025	8000.016843	9.776512	-0.057504	4.816077
281.747605	7999.872263	9.781517	-0.057489	4.816035
281.614020	7999.897617	9.786522	-0.057464	4.816043
281.705276	7999.890722	9.791527	-0.057481	4.816041
281.725341	7999.886811	9.796531	-0.057485	4.816040
281.639033	7999.885245	9.801536	-0.057469	4.816040
281.757714	7999.872438	9.806541	-0.057491	4.816035
281.692625	7999.916127	9.811546	-0.057479	4.816048
281.595770	7999.903687	9.816551	-0.057461	4.816045
281.706300	7999.869365	9.821555	-0.057481	4.816035
281.889645	7999.944265	9.826560	-0.057515	4.816055
281.696642	7999.864913	9.831565	-0.057479	4.816033
281.803676	7999.945908	9.836570	-0.057499	4.816056
281.779005	7999.894179	9.841575	-0.057495	4.816041
281.848570	7999.842022	9.846579	-0.057508	4.816026
281.810674	7999.968465	9.851584	-0.057501	4.816063
281.899730	7999.871791	9.856589	-0.057517	4.816034
281.977776	7999.889229	9.861594	-0.057532	4.816039
281.934299	7999.910874	9.866599	-0.057524	4.816045
281.819088	7999.881008	9.871603	-0.057502	4.816037
281.912721	7999.921163	9.876608	-0.057519	4.816049
281.828505	7999.860877	9.881613	-0.057504	4.816031
281.832287	7999.868422	9.886618	-0.057504	4.816034
281.574114	8000.010104	9.891623	-0.057456	4.816076
281.834129	7999.804352	9.896627	-0.057505	4.816015
281.782857	7999.919870	9.901632	-0.057495	4.816049
281.653552	7999.897227	9.906637	-0.057471	4.816043
281.696910	7999.915104	9.911642	-0.057479	4.816048
281.863538	7999.893551	9.916647	-0.057510	4.816041
281.932104	7999.812530	9.921651	-0.057523	4.816017
281.894391	7999.909063	9.926656	-0.057516	4.816045
281.969159	7999.882640	9.931661	-0.057530	4.816037
282.164412	7999.923569	9.936666	-0.057566	4.816048
282.024374	7999.891116	9.941671	-0.057540	4.816039
282.102360	7999.888254	9.946675	-0.057555	4.816038
281.896008	7999.940066	9.951680	-0.057516	4.816054
281.879289	7999.958992	9.956685	-0.057513	4.816060
282.164906	7999.833829	9.961690	-0.057566	4.816022
281.889911	7999.894013	9.966695	-0.057515	4.816041
282.099490	7999.809137	9.971699	-0.057554	4.816015
282.024095	7999.930628	9.976704	-0.057540	4.816051
282.010531	7999.864144	9.981709	-0.057537	4.816031
281.983408	7999.913862	9.986714	-0.057532	4.816046
281.961435	7999.899574	9.991719	-0.057528	4.816042
282.049398	7999.800743	9.996723	-0.057544	4.816013
282.082753	7999.944504	10.001728	-0.057551	4.816054
282.032364	7999.875215	10.006733	-0.057541	4.816035
282.090605	7999.817510	10.011738	-0.057552	4.816017
282.080544	7999.992534	10.016743	-0.057550	4.816069
282.096403	7999.858209	10.021747	-0.057553	4.816029
282.168678	7999.855244	10.026752	-0.057567	4.816028
282.346612	7999.874492	10.031757	-0.057600	4.816033
282.245327	7999.922867	10.036762	-0.057581	4.816047
282.155545	7999.850727	10.041767	-0.057564	4.816027
282.246779	7999.790416	10.046771	-0.057581	4.816009
282.115173	7999.886316	10.051776	-0.057557	4.816037
282.100954	7999.872168	10.056781	-0.057554	4.816033
282.249275	7999.909042	10.061786	-0.057582	4.816043
282.208204	7999.901886	10.066791	-0.057574	4.816041
282.078406	7999.795903	10.071795	-0.057550	4.816011
281.979471	7999.951154	10.076800	-0.057531	4.816057
282.179230	7999.894946	10.081805	-0.057568	4.816040
282.059480	7999.941918	10.086810	-0.057546	4.816054
281.971918	7999.886912	10.091815	-0.057530	4.816038
282.124347	7999.782839	10.096819	-0.057558	4.816007
282.123501	8000.005038	10.101824	-0.057558	4.816072
282.166903	7999.875484	10.106829	-0.057566	4.816034
282.348384	7999.786894	10.111834	-0.057600	4.816007
282.317000	7999.954055	10.116839	-0.057594	4.816056
282.311811	7999.822552	10.121843	-0.057593	4.816018
282.134544	7999.910147	10.126848	-0.057560	4.816044
282.150968	7999.913648	10.131853	-0.057563	4.816045
282.337434	7999.837969	10.136858	-0.057598	4.816022
282.042900	7999.904208	10.141863	-0.057543	4.816043
282.143711	7999.884666	10.146867	-0.057562	4.816037
282.080747	7999.860020	10.151872	-0.057550	4.816030
282.098492	7999.845383	10.156877	-0.057553	4.816025
282.315085	7999.867469	10.161882	-0.057593	4.816031
282.356257	7999.910948	10.166887	-0.057601	4.816043
282.361835	7999.861903	10.171891	-0.057602	4.816029
282.203737	7999.929547	10.176896	-0.057573	4.816049
282.379163	7999.797045	10.181901	-0.057605	4.816010
282.419958	7999.925985	10.186906	-0.057613	4.816047
282.133507	7999.875920	10.191911	-0.057560	4.816034
282.444127	7999.890096	10.196915	-0.057617	4.816037
282.444095	7999.886888	10.201920	-0.057617	4.816036
282.386424	7999.832424	10.206925	-0.057607	4.816020
282.204378	7999.863310	10.211930	-0.057573	4.816030
282.147586	7999.946678	10.216935	-0.057562	4.816055
282.271521	7999.847430	10.221939	-0.057585	4.816025
282.062170	7999.835087	10.226944	-0.057546	4.816023
282.016381	7999.881263	10.231949	-0.057538	4.816036
282.271348	7999.942505	10.236954	-0.057585	4.816053
282.313815	7999.818277	10.241959	-0.057593	4.816016
282.368617	7999.822473	10.246963	-0.057603	4.816017
282.471775	7999.955749	10.251968	-0.057622	4.816056
282.253989	7999.883425	10.256973	-0.057582	4.816036
282.331518	7999.823933	10.261978	-0.057596	4.816018
282.148728	7999.917838	10.266983	-0.057562	4.816046
282.387434	7999.856993	10.271987	-0.057607	4.816027
282.227820	7999.923541	10.276992	-0.057577	4.816048
282.175848	7999.797601	10.281997	-0.057567	4.816011
282.246207	7999.892889	10.287002	-0.057580	4.816039
282.212782	7999.931811	10.292007	-0.057574	4.816050
282.376936	7999.808720	10.297011	-0.057604	4.816013
282.234362	7999.932199	10.302016	-0.057578	4.816050
282.168011	7999.834843	10.307021	-0.057566	4.816022
282.148284	7999.912473	10.312026	-0.057562	4.816045
282.228392	7999.894694	10.317031	-0.057577	4.816039
282.431744	7999.852439	10.322035	-0.057615	4.816026
282.485367	7999.894007	10.327040	-0.057625	4.816038
282.400331	7999.805927	10.332045	-0.057609	4.816012
282.559725	7999.979752	10.337050	-0.057638	4.816062
282.345775	7999.822029	10.342055	-0.057599	4.816017
282.327133	7999.851603	10.347059	-0.057595	4.816026
282.494180	7999.897363	10.352064	-0.057626	4.816039
282.473049	7999.822194	10.357069	-0.057622	4.816017
282.416006	7999.872439	10.362074	-0.057612	4.816032
282.297226	7999.896994	10.367079	-0.057589	4.816040
282.452948	7999.825030	10.372083	-0.057618	4.816018
282.421062	7999.940901	10.377088	-0.057612	4.816052
282.400810	7999.816603	10.382093	-0.057609	4.816015
282.478156	7999.831892	10.387098	-0.057623	4.816020
282.237344	7999.961069	10.392103	-0.057578	4.816059
282.394717	7999.889136	10.397107	-0.057607	4.816037
282.544141	7999.850177	10.402112	-0.057635	4.816025
282.603913	7999.864079	10.407117	-0.057646	4.816028
282.517575	7999.871060	10.412122	-0.057630	4.816031
282.387548	7999.845197	10.417127	-0.057606	4.816024
282.657855	7999.880009	10.422131	-0.057656	4.816033
282.566693	7999.940320	10.427136	-0.057639	4.816051
282.533871	7999.829683	10.432141	-0.057633	4.816019
282.638218	7999.892469	10.437146	-0.057653	4.816036
282.704838	7999.850941	10.442151	-0.057665	4.816024
282.618021	7999.889963	10.447155	-0.057649	4.816036
282.527716	7999.885119	10.452160	-0.057632	4.816035
282.523621	7999.905342	10.457165	-0.057631	4.816041
282.614042	7999.882407	10.462170	-0.057648	4.816034
282.545843	7999.841640	10.467175	-0.057635	4.816022
282.665232	7999.911110	10.472179	-0.057658	4.816042
282.467932	7999.876549	10.477184	-0.057621	4.816033
282.530671	7999.895847	10.482189	-0.057633	4.816038
282.543330	7999.934535	10.487194	-0.057635	4.816049
282.462587	7999.907429	10.492199	-0.057620	4.816042
282.369457	7999.983730	10.497203	-0.057603	4.816064
282.790656	7999.909100	10.502208	-0.057681	4.816040
282.694146	7999.865683	10.507213	-0.057663	4.816028
282.604039	7999.886483	10.512218	-0.057646	4.816035
282.290265	7999.813488	10.517223	-0.057588	4.816015
282.635278	7999.844312	10.522227	-0.057652	4.816022
282.549565	7999.964550	10.527232	-0.057636	4.816058
282.489625	7999.847011	10.532237	-0.057625	4.816024
282.599694	7999.869303	10.537242	-0.057645	4.816030
282.530272	7999.916119	10.542247	-0.057632	4.816044
282.639754	7999.821950	10.547251	-0.057653	4.816016
282.584178	7999.827351	10.552256	-0.057642	4.816018
282.490022	7999.919658	10.557261	-0.057625	4.816045
282.481615	7999.891727	10.562266	-0.057623	4.816037
282.304464	7999.901334	10.567271	-0.057590	4.816041
282.520256	7999.860373	10.572275	-0.057630	4.816028
282.555713	7999.815075	10.577280	-0.057637	4.816014
282.621918	7999.914562	10.582285	-0.057649	4.816043
282.695938	7999.892399	10.587290	-0.057663	4.816036
282.752322	7999.863505	10.592295	-0.057673	4.816027
282.571695	7999.863434	10.597299	-0.057640	4.816028
282.517231	7999.932957	10.602304	-0.057630	4.816049
282.568350	7999.836662	10.607309	-0.057639	4.816020
282.871788	7999.844298	10.612314	-0.057696	4.816021
282.670873	7999.914370	10.617319	-0.057658	4.816043
282.776545	7999.830816	10.622323	-0.057678	4.816018
282.790668	7999.840685	10.627328	-0.057680	4.816020
282.612563	7999.875916	10.632333	-0.057647	4.816032
282.849065	7999.943235	10.637338	-0.057691	4.816050
282.890222	7999.871331	10.642343	-0.057699	4.816029
282.642404	7999.861495	10.647347	-0.057653	4.816027
282.657117	7999.844667	10.652352	-0.057655	4.816022
282.767011	7999.902212	10.657357	-0.057676	4.816039
282.756508	7999.844328	10.662362	-0.057674	4.816022
282.670320	7999.845969	10.667367	-0.057658	4.816023
282.771190	7999.839250	10.672371	-0.057677	4.816020
282.784448	7999.968760	10.677376	-0.057679	4.816058
282.661116	7999.804132	10.682381	-0.057656	4.816010
282.847972	7999.938926	10.687386	-0.057691	4.816049
282.942982	7999.877614	10.692391	-0.057709	4.816030
282.709673	7999.846673	10.697395	-0.057665	4.816023
282.686054	7999.935986	10.702400	-0.057661	4.816049
282.802878	7999.787463	10.707405	-0.057682	4.816005
282.899486	7999.883229	10.712410	-0.057700	4.816032
282.708077	7999.872279	10.717415	-0.057665	4.816030
282.864784	7999.915716	10.722419	-0.057694	4.816042
282.988767	7999.884843	10.727424	-0.057717	4.816032
282.772688	7999.826437	10.732429	-0.057677	4.816016
282.743148	7999.870771	10.737434	-0.057671	4.816030
282.852473	7999.918691	10.742439	-0.057692	4.816043
282.883904	7999.841269	10.747443	-0.057697	4.816020
282.756425	7999.873144	10.752448	-0.057674	4.816030
282.808241	7999.869808	10.757453	-0.057683	4.816029
282.906058	7999.874785	10.762458	-0.057701	4.816030
282.802651	7999.915643	10.767463	-0.057682	4.816042
282.886310	7999.811390	10.772467	-0.057698	4.816011
282.951965	7999.858519	10.777472	-0.057710	4.816025
282.718536	7999.869242	10.782477	-0.057666	4.816029
282.798150	7999.842907	10.787482	-0.057681	4.816021
282.971136	7999.883434	10.792487	-0.057714	4.816032
283.001830	7999.859416	10.797491	-0.057719	4.816025
282.973368	7999.887744	10.802496	-0.057714	4.816033
282.874410	7999.862445	10.807501	-0.057695	4.816026
282.930571	7999.890170	10.812506	-0.057706	4.816034
282.950890	7999.813615	10.817511	-0.057710	4.816012
283.027207	7999.890851	10.822515	-0.057724	4.816034
283.060543	7999.852993	10.827520	-0.057730	4.816023
282.940482	7999.839062	10.832525	-0.057708	4.816019
282.925571	7999.880457	10.837530	-0.057705	4.816031
283.209201	7999.941153	10.842535	-0.057758	4.816048
283.132136	7999.851079	10.847539	-0.057743	4.816022
283.097870	7999.906011	10.852544	-0.057737	4.816038
283.041392	7999.847294	10.857549	-0.057726	4.816021
283.153422	7999.855734	10.862554	-0.057747	4.816023
282.897382	7999.919465	10.867559	-0.057700	4.816043
283.062528	7999.857288	10.872563	-0.057730	4.816024
283.191276	7999.850005	10.877568	-0.057754	4.816021
283.081454	7999.859764	10.882573	-0.057734	4.816025
282.965102	7999.864063	10.887578	-0.057712	4.816026
282.886656	7999.906442	10.892583	-0.057697	4.816039
282.961450	7999.850105	10.897587	-0.057711	4.816022
282.929474	7999.864481	10.902592	-0.057705	4.816027
282.985237	7999.855875	10.907597	-0.057716	4.816024
283.117477	7999.958698	10.912602	-0.057740	4.816053
282.957799	7999.871400	10.917607	-0.057711	4.816029
283.050343	7999.885897	10.922611	-0.057728	4.816032
283.096650	7999.884598	10.927616	-0.057736	4.816032
283.000723	7999.831576	10.932621	-0.057719	4.816017
283.012982	7999.894830	10.937626	-0.057721	4.816035
282.938908	7999.938356	10.942631	-0.057707	4.816048
283.088650	7999.890857	10.947635	-0.057735	4.816034
282.877773	7999.873143	10.952640	-0.057696	4.816030
282.844326	7999.858646	10.957645	-0.057689	4.816025
283.172456	7999.914807	10.962650	-0.057750	4.816040
282.870003	7999.870861	10.967655	-0.057694	4.816029
282.681094	7999.856751	10.972659	-0.057659	4.816026
282.919022	7999.890977	10.977664	-0.057703	4.816035
283.079666	7999.924870	10.982669	-0.057733	4.816044
283.222911	7999.869774	10.987674	-0.057760	4.816027
283.121457	7999.839087	10.992679	-0.057741	4.816018
282.983826	7999.904966	10.997683	-0.057715	4.816038
283.058983	7999.879617	11.002688	-0.057729	4.816030
282.957133	7999.917299	11.007693	-0.057710	4.816042
283.058872	7999.917005	11.012698	-0.057729	4.816041
282.905795	7999.837306	11.017703	-0.057701	4.816019
282.765024	7999.894580	11.022707	-0.057674	4.816036
282.910747	7999.857691	11.027712	-0.057701	4.816025
282.724798	7999.866071	11.032717	-0.057667	4.816028
282.694495	7999.911459	11.037722	-0.057661	4.816042
282.916326	7999.843899	11.042727	-0.057702	4.816021
283.243297	7999.984441	11.047731	-0.057763	4.816060
283.110912	7999.906184	11.052736	-0.057739	4.816038
283.050524	7999.834575	11.057741	-0.057727	4.816017
283.302747	7999.826326	11.062746	-0.057774	4.816014
283.184749	7999.822048	11.067751	-0.057752	4.816013
283.020135	7999.902395	11.072755	-0.057722	4.816037
282.976176	7999.919758	11.077760	-0.057714	4.816043
282.975257	7999.945381	11.082765	-0.057713	4.816050
283.009865	7999.850922	11.087770	-0.057720	4.816022
283.043845	7999.853673	11.092775	-0.057726	4.816023
283.098759	7999.855736	11.097779	-0.057736	4.816023
283.000179	7999.924459	11.102784	-0.057718	4.816044
282.949517	7999.791062	11.107789	-0.057708	4.816005
283.145871	7999.921756	11.112794	-0.057745	4.816042
283.064948	7999.848706	11.117799	-0.057730	4.816021
283.083535	7999.840495	11.122803	-0.057733	4.816019
282.952127	7999.947084	11.127808	-0.057709	4.816051
283.044241	7999.867556	11.132813	-0.057726	4.816027
283.055770	7999.884858	11.137818	-0.057728	4.816032
282.951681	7999.835961	11.142823	-0.057709	4.816018
283.055213	7999.892323	11.147827	-0.057728	4.816034
283.165211	7999.852649	11.152832	-0.057748	4.816022
283.188887	7999.805001	11.157837	-0.057753	4.816008
283.265549	7999.970918	11.162842	-0.057767	4.816056
283.221552	7999.879307	11.167847	-0.057759	4.816030
283.268424	7999.851309	11.172851	-0.057768	4.816021
283.354916	7999.895611	11.177856	-0.057784	4.816034
283.060030	7999.852870	11.182861	-0.057729	4.816023
283.087172	7999.900368	11.187866	-0.057734	4.816036
282.881156	7999.885948	11.192871	-0.057695	4.816033
283.001760	7999.884928	11.197875	-0.057718	4.816032
283.031028	7999.908961	11.202880	-0.057723	4.816039
282.885250	7999.892427	11.207885	-0.057696	4.816035
283.119570	8000.021674	11.212890	-0.057740	4.816072
283.161869	7999.900645	11.217895	-0.057748	4.816036
283.020031	7999.918370	11.222899	-0.057721	4.816042
282.975682	7999.927180	11.227904	-0.057713	4.816045
283.150495	7999.850220	11.232909	-0.057745	4.816021
283.364400	7999.913926	11.237914	-0.057785	4.816039
283.099281	7999.892023	11.242919	-0.057736	4.816034
283.097386	7999.844979	11.247923	-0.057735	4.816020
283.301801	7999.940564	11.252928	-0.057774	4.816047
283.339739	7999.785268	11.257933	-0.057781	4.816001
283.468641	7999.853843	11.262938	-0.057805	4.816021
283.447237	7999.931444	11.267943	-0.057801	4.816044
283.518460	7999.884657	11.272947	-0.057814	4.816030
283.547354	7999.918299	11.277952	-0.057819	4.816039
283.459526	7999.849397	11.282957	-0.057803	4.816020
283.455078	7999.895255	11.287962	-0.057802	4.816033
283.049601	7999.877218	11.292967	-0.057726	4.816030
283.405691	7999.879399	11.297971	-0.057793	4.816029
283.578146	7999.884662	11.302976	-0.057825	4.816029
283.349167	7999.904012	11.307981	-0.057782	4.816036
283.290388	7999.956363	11.312986	-0.057771	4.816052
283.391924	7999.924015	11.317991	-0.057790	4.816042
283.383686	7999.907838	11.322995	-0.057789	4.816037
283.258854	7999.924804	11.328000	-0.057765	4.816043
283.229197	7999.860162	11.333005	-0.057760	4.816024
283.362144	7999.888212	11.338010	-0.057785	4.816031
283.211871	7999.943178	11.343015	-0.057757	4.816048
283.325121	7999.887538	11.348019	-0.057778	4.816031
283.270365	7999.905774	11.353024	-0.057767	4.816037
283.110399	7999.848385	11.358029	-0.057738	4.816021
283.310705	7999.875519	11.363034	-0.057775	4.816028
283.365189	7999.880779	11.368039	-0.057785	4.816029
283.118823	7999.905156	11.373043	-0.057739	4.816038
283.066391	7999.903136	11.378048	-0.057729	4.816037
283.198375	7999.899117	11.383053	-0.057754	4.816035
283.404834	7999.919953	11.388058	-0.057792	4.816040
283.164279	7999.893154	11.393063	-0.057748	4.816034
283.124613	7999.956535	11.398067	-0.057740	4.816053
283.347642	7999.936005	11.403072	-0.057782	4.816045
283.164743	7999.851491	11.408077	-0.057748	4.816022
283.118182	7999.908337	11.413082	-0.057739	4.816039
283.236526	7999.872020	11.418087	-0.057761	4.816027
283.330761	7999.874795	11.423091	-0.057778	4.816028
283.199762	7999.909811	11.428096	-0.057754	4.816039
283.254156	7999.865925	11.433101	-0.057764	4.816025
283.383914	7999.891780	11.438106	-0.057788	4.816032
283.018057	7999.908649	11.443111	-0.057720	4.816039
283.174487	7999.933919	11.448115	-0.057749	4.816046
283.107857	7999.916684	11.453120	-0.057737	4.816041
283.057235	7999.876235	11.458125	-0.057727	4.816030
283.158896	7999.890897	11.463130	-0.057746	4.816033
283.190532	7999.889332	11.468135	-0.057752	4.816033
283.260465	7999.971795	11.473139	-0.057765	4.816056
283.350217	7999.863378	11.478144	-0.057782	4.816024
283.318869	7999.832894	11.483149	-0.057776	4.816015
283.509490	7999.887631	11.488154	-0.057811	4.816030
283.371795	7999.852013	11.493159	-0.057786	4.816021
283.384925	7999.838360	11.498163	-0.057788	4.816017
283.359303	7999.878492	11.503168	-0.057783	4.816029
283.298885	7999.920130	11.508173	-0.057772	4.816041
283.449492	7999.857689	11.513178	-0.057800	4.816022
283.488175	7999.826337	11.518183	-0.057807	4.816013
283.544025	7999.905340	11.523187	-0.057818	4.816035
283.471339	7999.859148	11.528192	-0.057804	4.816022
283.279316	7999.828956	11.533197	-0.057768	4.816015
283.402641	7999.858968	11.538202	-0.057791	4.816023
283.376537	7999.962126	11.543207	-0.057787	4.816053
283.319654	7999.816862	11.548211	-0.057776	4.816011
283.496511	7999.867076	11.553216	-0.057809	4.816025
283.375956	7999.837110	11.558221	-0.057786	4.816016
283.549088	7999.910761	11.563226	-0.057819	4.816037
283.452339	7999.973108	11.568231	-0.057801	4.816056
283.534827	7999.851738	11.573235	-0.057816	4.816020
283.659024	7999.902066	11.578240	-0.057839	4.816034
283.616554	7999.883132	11.583245	-0.057831	4.816029
283.624516	7999.893958	11.588250	-0.057833	4.816032
283.510196	7999.834191	11.593255	-0.057811	4.816015
283.460945	7999.948681	11.598259	-0.057802	4.816049
283.646853	7999.852692	11.603264	-0.057837	4.816020
283.444685	7999.802016	11.608269	-0.057799	4.816006
283.596781	7999.867806	11.613274	-0.057827	4.816024
283.552440	7999.979181	11.618279	-0.057819	4.816057
283.461981	7999.883521	11.623283	-0.057802	4.816030
283.404430	7999.892091	11.628288	-0.057791	4.816032
282.966629	7999.924749	11.633293	-0.057710	4.816044
283.358706	7999.922242	11.638298	-0.057783	4.816041
283.617127	7999.850003	11.643303	-0.057831	4.816019
283.571974	7999.909012	11.648307	-0.057823	4.816036
283.794408	7999.871377	11.653312	-0.057864	4.816024
283.531100	7999.826002	11.658317	-0.057815	4.816012
283.541843	7999.835811	11.663322	-0.057817	4.816015
283.457694	7999.875950	11.668327	-0.057801	4.816027
283.455234	7999.930391	11.673331	-0.057801	4.816043
283.485759	7999.909576	11.678336	-0.057806	4.816037
283.391292	7999.858716	11.683341	-0.057789	4.816023
283.578683	7999.870659	11.688346	-0.057824	4.816025
283.401435	7999.967871	11.693351	-0.057791	4.816054
283.398481	7999.879140	11.698355	-0.057790	4.816029
283.671557	7999.856313	11.703360	-0.057841	4.816020
283.482094	7999.918047	11.708365	-0.057806	4.816040
283.308113	7999.875360	11.713370	-0.057773	4.816028
283.426887	7999.880717	11.718375	-0.057795	4.816029
283.453101	7999.804268	11.723379	-0.057800	4.816006
283.527494	7999.869718	11.728384	-0.057814	4.816025
283.574374	7999.936806	11.733389	-0.057823	4.816045
283.755706	7999.861033	11.738394	-0.057856	4.816021
283.717981	7999.915903	11.743399	-0.057849	4.816038
283.602804	7999.809111	11.748403	-0.057828	4.816007
283.462721	7999.871741	11.753408	-0.057802	4.816026
283.682888	7999.868253	11.758413	-0.057843	4.816024
283.703769	7999.938075	11.763418	-0.057847	4.816044
283.403011	7999.911251	11.768423	-0.057791	4.816038
283.565649	7999.779584	11.773427	-0.057821	4.815999
283.590659	7999.927472	11.778432	-0.057826	4.816042
283.484246	7999.861438	11.783437	-0.057806	4.816023
283.755844	7999.811874	11.788442	-0.057856	4.816007
283.792616	7999.922583	11.793447	-0.057863	4.816039
283.718934	7999.756714	11.798451	-0.057849	4.815991
283.945743	7999.928562	11.803456	-0.057892	4.816040
283.695807	7999.902659	11.808461	-0.057845	4.816034
283.685794	7999.891792	11.813466	-0.057843	4.816031
283.623108	7999.840440	11.818471	-0.057832	4.816016
283.858652	7999.814795	11.823475	-0.057875	4.816007
283.708035	7999.878302	11.828480	-0.057847	4.816027
283.518613	7999.868455	11.833485	-0.057812	4.816025
283.720932	7999.866780	11.838490	-0.057850	4.816023
283.669293	7999.885073	11.843495	-0.057840	4.816029
283.758731	7999.896309	11.848499	-0.057857	4.816032
283.807608	7999.819202	11.853504	-0.057866	4.816009
283.853717	7999.822173	11.858509	-0.057874	4.816010
283.819386	7999.887789	11.863514	-0.057868	4.816029
283.689289	7999.971967	11.868519	-0.057844	4.816054
283.672371	7999.838111	11.873523	-0.057840	4.816015
283.775057	7999.874160	11.878528	-0.057860	4.816025
283.691642	7999.869440	11.883533	-0.057844	4.816024
283.720535	7999.925518	11.888538	-0.057849	4.816040
283.641925	7999.805501	11.893543	-0.057835	4.816006
283.817089	7999.845001	11.898547	-0.057867	4.816016
283.623476	7999.939779	11.903552	-0.057831	4.816045
283.730843	7999.895784	11.908557	-0.057851	4.816032
283.720011	7999.789816	11.913562	-0.057849	4.816001
283.728722	7999.848734	11.918567	-0.057851	4.816018
283.560056	7999.941828	11.923571	-0.057819	4.816046
283.798331	7999.839309	11.928576	-0.057864	4.816015
283.753926	7999.819271	11.933581	-0.057855	4.816009
283.744105	7999.873579	11.938586	-0.057854	4.816025
283.651057	7999.844112	11.943591	-0.057836	4.816017
283.618070	7999.945008	11.948595	-0.057830	4.816047
283.747644	7999.821288	11.953600	-0.057854	4.816010
283.833673	7999.878402	11.958605	-0.057870	4.816026
283.851646	7999.806076	11.963610	-0.057874	4.816005
283.714194	7999.843112	11.968615	-0.057848	4.816016
283.687787	7999.920624	11.973619	-0.057843	4.816039
283.856825	7999.861721	11.978624	-0.057875	4.816021
283.529556	7999.856853	11.983629	-0.057814	4.816021
283.609293	7999.840135	11.988634	-0.057828	4.816016
283.698873	7999.855647	11.993639	-0.057845	4.816020
283.756168	7999.918651	11.998643	-0.057856	4.816038
283.678927	7999.841393	12.003648	-0.057841	4.816016
283.800613	7999.815820	12.008653	-0.057864	4.816008
284.007157	7999.961660	12.013658	-0.057902	4.816049
283.836802	7999.811131	12.018663	-0.057871	4.816006
283.577611	7999.891900	12.023667	-0.057822	4.816031
283.888010	7999.834493	12.028672	-0.057880	4.816013
283.788181	7999.878621	12.033677	-0.057862	4.816026
283.845572	7999.839062	12.038682	-0.057872	4.816015
283.817799	7999.857788	12.043687	-0.057867	4.816020
283.819912	7999.810816	12.048691	-0.057867	4.816006
283.886891	7999.891089	12.053696	-0.057880	4.816030
283.804909	7999.851139	12.058701	-0.057865	4.816018
283.879501	7999.889883	12.063706	-0.057878	4.816029
283.918248	7999.817934	12.068711	-0.057886	4.816008
283.942198	7999.841872	12.073715	-0.057890	4.816015
284.057114	7999.879211	12.078720	-0.057911	4.816025
283.935070	7999.907979	12.083725	-0.057889	4.816034
283.822299	7999.809778	12.088730	-0.057868	4.816006
283.712350	7999.825945	12.093735	-0.057847	4.816011
283.713303	7999.900747	12.098739	-0.057847	4.816033
283.890967	7999.877258	12.103744	-0.057880	4.816025
283.711316	7999.800280	12.108749	-0.057847	4.816004
283.993262	7999.840648	12.113754	-0.057899	4.816014
283.962607	7999.926630	12.118759	-0.057894	4.816040
283.806234	7999.830843	12.123763	-0.057865	4.816012
283.892224	7999.823854	12.128768	-0.057881	4.816010
283.852120	7999.802825	12.133773	-0.057873	4.816004
283.894284	7999.922179	12.138778	-0.057881	4.816039
283.793979	7999.847708	12.143783	-0.057862	4.816017
283.930050	7999.798892	12.148787	-0.057888	4.816002
284.111805	7999.923983	12.153792	-0.057921	4.816038
283.986280	7999.802045	12.158797	-0.057898	4.816003
284.065015	7999.847275	12.163802	-0.057913	4.816016
284.000379	7999.911273	12.168807	-0.057901	4.816035
283.971696	7999.882973	12.173811	-0.057895	4.816027
284.145692	7999.859418	12.178816	-0.057928	4.816019
284.047603	7999.810628	12.183821	-0.057909	4.816005
284.066830	7999.829138	12.188826	-0.057913	4.816010
283.894762	7999.898666	12.193831	-0.057881	4.816032
283.889999	7999.787466	12.198835	-0.057880	4.815999
284.070445	7999.867660	12.203840	-0.057914	4.816022
283.971936	7999.916087	12.208845	-0.057895	4.816036
284.013744	7999.830304	12.213850	-0.057903	4.816011
283.980410	7999.918374	12.218855	-0.057897	4.816037
283.788929	7999.785625	12.223859	-0.057861	4.815999
284.024447	7999.909554	12.228864	-0.057905	4.816034
284.003713	7999.870714	12.233869	-0.057901	4.816023
283.916577	7999.783661	12.238874	-0.057885	4.815998
283.970317	7999.971602	12.243879	-0.057895	4.816053
283.961487	7999.884901	12.248883	-0.057893	4.816027
284.120544	7999.863211	12.253888	-0.057923	4.816020
283.918420	7999.874501	12.258893	-0.057885	4.816025
283.814893	7999.889716	12.263898	-0.057866	4.816030
283.999402	7999.886651	12.268903	-0.057900	4.816028
284.050750	7999.874760	12.273907	-0.057910	4.816024
284.056643	7999.855634	12.278912	-0.057911	4.816018
283.907912	7999.829430	12.283917	-0.057883	4.816011
283.878447	7999.919707	12.288922	-0.057878	4.816038
283.976402	7999.832806	12.293927	-0.057896	4.816012
284.095614	7999.765521	12.298931	-0.057918	4.815992
284.103550	7999.925922	12.303936	-0.057919	4.816039
283.863287	7999.770920	12.308941	-0.057875	4.815995
284.011204	7999.938133	12.313946	-0.057902	4.816043
284.080519	7999.882764	12.318951	-0.057915	4.816026
284.043797	7999.763505	12.323955	-0.057908	4.815991
284.061905	7999.929432	12.328960	-0.057912	4.816040
283.940658	7999.812914	12.333965	-0.057889	4.816006
283.933014	7999.821321	12.338970	-0.057887	4.816009
283.818473	7999.839541	12.343975	-0.057866	4.816015
283.864571	7999.920505	12.348979	-0.057875	4.816038
283.966661	7999.849704	12.353984	-0.057894	4.816017
283.825666	7999.814026	12.358989	-0.057867	4.816007
284.007679	7999.925232	12.363994	-0.057901	4.816039
283.949883	7999.793839	12.368999	-0.057891	4.816001
284.071577	7999.885789	12.374003	-0.057913	4.816027
284.200250	7999.877438	12.379008	-0.057937	4.816024
284.243327	7999.833345	12.384013	-0.057945	4.816011
284.218349	7999.854258	12.389018	-0.057940	4.816017
284.118130	7999.844960	12.394023	-0.057922	4.816015
283.931878	7999.902478	12.399027	-0.057887	4.816033
284.054379	7999.860895	12.404032	-0.057910	4.816020
284.057536	7999.800052	12.409037	-0.057910	4.816002
284.166266	7999.868263	12.414042	-0.057931	4.816021
284.040910	7999.967485	12.419047	-0.057907	4.816051
283.927065	7999.764561	12.424051	-0.057886	4.815992
283.859233	7999.880852	12.429056	-0.057873	4.816027
284.031040	7999.854051	12.434061	-0.057905	4.816018
283.990086	7999.903521	12.439066	-0.057898	4.816033
283.831886	7999.805564	12.444071	-0.057868	4.816005
283.837753	7999.898618	12.449075	-0.057869	4.816032
284.399812	7999.871418	12.454080	-0.057974	4.816021
283.994926	7999.804243	12.459085	-0.057899	4.816004
284.051469	7999.880054	12.464090	-0.057909	4.816025
284.212929	7999.875502	12.469095	-0.057939	4.816023
284.041357	7999.817901	12.474099	-0.057907	4.816007
284.020597	7999.876284	12.479104	-0.057903	4.816025
284.007348	7999.847195	12.484109	-0.057901	4.816016
284.269859	7999.803877	12.489114	-0.057950	4.816002
284.102484	7999.917295	12.494119	-0.057919	4.816036
284.164516	7999.884230	12.499123	-0.057930	4.816026
284.146247	7999.799494	12.504128	-0.057927	4.816001
283.951526	7999.866474	12.509133	-0.057890	4.816022
284.025624	7999.881706	12.514138	-0.057904	4.816026
284.246831	7999.857938	12.519143	-0.057945	4.816018
284.014925	7999.875098	12.524147	-0.057902	4.816024
283.931543	7999.823370	12.529152	-0.057887	4.816010
284.150580	7999.865803	12.534157	-0.057927	4.816021
284.152798	7999.901099	12.539162	-0.057928	4.816031
284.144697	7999.800521	12.544167	-0.057926	4.816002
284.144745	7999.872103	12.549171	-0.057926	4.816023
284.466607	7999.840545	12.554176	-0.057986	4.816012
284.212790	7999.860513	12.559181	-0.057939	4.816019
284.237181	7999.803261	12.564186	-0.057943	4.816002
284.277485	7999.877709	12.569191	-0.057951	4.816024
284.117605	7999.885492	12.574195	-0.057921	4.816027
284.091145	7999.805949	12.579200	-0.057916	4.816004
284.146471	7999.862507	12.584205	-0.057926	4.816020
284.136829	7999.828142	12.589210	-0.057925	4.816010
284.106593	7999.876738	12.594215	-0.057919	4.816024
283.968019	7999.867813	12.599219	-0.057893	4.816022
284.097294	7999.807121	12.604224	-0.057917	4.816004
283.993655	7999.876822	12.609229	-0.057898	4.816025
284.019139	7999.799290	12.614234	-0.057903	4.816002
284.059638	7999.967760	12.619239	-0.057910	4.816051
284.133522	7999.841960	12.624243	-0.057924	4.816014
284.255301	7999.819594	12.629248	-0.057947	4.816007
284.037347	7999.915000	12.634253	-0.057906	4.816036
284.187913	7999.804480	12.639258	-0.057934	4.816003
284.244051	7999.808702	12.644263	-0.057944	4.816004
284.204002	7999.958617	12.649267	-0.057937	4.816048
284.274297	7999.832752	12.654272	-0.057950	4.816010
284.261011	7999.881655	12.659277	-0.057948	4.816025
284.169744	7999.867177	12.664282	-0.057931	4.816021
284.197080	7999.859124	12.669287	-0.057936	4.816019
284.277334	7999.859510	12.674291	-0.057951	4.816018
283.979364	7999.881882	12.679296	-0.057895	4.816026
283.855322	7999.875357	12.684301	-0.057872	4.816025
283.993178	7999.788111	12.689306	-0.057898	4.815999
284.155087	7999.879723	12.694311	-0.057928	4.816025
283.963902	7999.909373	12.699315	-0.057892	4.816035
284.264829	7999.863547	12.704320	-0.057948	4.816020
284.228164	7999.832966	12.709325	-0.057941	4.816011
284.176761	7999.866220	12.714330	-0.057932	4.816021
284.022064	7999.860208	12.719335	-0.057903	4.816020
284.237598	7999.848089	12.724339	-0.057943	4.816015
284.118996	7999.858757	12.729344	-0.057921	4.816019
284.040749	7999.881909	12.734349	-0.057906	4.816026
284.136190	7999.839835	12.739354	-0.057924	4.816013
284.159077	7999.868027	12.744359	-0.057928	4.816021
284.173236	7999.867213	12.749363	-0.057931	4.816021
284.056933	7999.857624	12.754368	-0.057909	4.816019
284.187896	7999.913417	12.759373	-0.057934	4.816035
284.305267	7999.810842	12.764378	-0.057955	4.816004
284.142505	7999.848487	12.769383	-0.057925	4.816016
284.196263	7999.851597	12.774387	-0.057935	4.816016
284.257173	7999.967019	12.779392	-0.057946	4.816050
284.053799	7999.819095	12.784397	-0.057909	4.816008
284.375945	7999.818526	12.789402	-0.057968	4.816006
284.076887	7999.890024	12.794407	-0.057913	4.816028
284.147264	7999.793007	12.799411	-0.057926	4.816000
284.226882	7999.855348	12.804416	-0.057941	4.816017
284.082324	7999.976658	12.809421	-0.057914	4.816054
284.283221	7999.864914	12.814426	-0.057951	4.816020
284.267307	7999.863555	12.819431	-0.057948	4.816020
284.244993	7999.879175	12.824435	-0.057944	4.816024
284.308084	7999.835445	12.829440	-0.057956	4.816011
284.136607	7999.878274	12.834445	-0.057924	4.816025
284.209035	7999.771679	12.839450	-0.057937	4.815993
284.216347	7999.968394	12.844455	-0.057939	4.816050
284.143170	7999.852747	12.849459	-0.057925	4.816017
284.398916	7999.789007	12.854464	-0.057973	4.815997
284.221342	7999.829589	12.859469	-0.057939	4.816010
284.296312	7999.924966	12.864474	-0.057953	4.816037
284.168646	7999.838245	12.869479	-0.057930	4.816013
284.236419	7999.856567	12.874483	-0.057942	4.816018
284.200659	7999.836686	12.879488	-0.057936	4.816012
284.139182	7999.926383	12.884493	-0.057924	4.816039
284.141617	7999.824928	12.889498	-0.057925	4.816009
284.151918	7999.811224	12.894503	-0.057926	4.816005
284.172676	7999.878908	12.899507	-0.057930	4.816025
284.242031	7999.811787	12.904512	-0.057943	4.816005
284.205060	7999.995947	12.909517	-0.057936	4.816059
284.214144	7999.790978	12.914522	-0.057938	4.815999
284.019426	7999.804540	12.919527	-0.057902	4.816004
284.068626	7999.897312	12.924531	-0.057911	4.816030
284.226007	7999.868113	12.929536	-0.057940	4.816021
284.051116	7999.868144	12.934541	-0.057908	4.816022
283.975698	7999.809082	12.939546	-0.057893	4.816005
284.274436	7999.812362	12.944551	-0.057949	4.816005
284.266310	7999.958583	12.949555	-0.057948	4.816047
284.509776	7999.787780	12.954560	-0.057993	4.815996
284.126144	7999.883386	12.959565	-0.057921	4.816026
284.192498	7999.827963	12.964570	-0.057934	4.816010
284.362854	7999.916524	12.969575	-0.057966	4.816035
284.340645	7999.782570	12.974579	-0.057961	4.815995
284.423156	7999.834279	12.979584	-0.057977	4.816010
284.083088	7999.900760	12.984589	-0.057913	4.816031
284.151879	7999.882775	12.989594	-0.057926	4.816026
284.284953	7999.837109	12.994599	-0.057951	4.816012
284.302870	7999.848117	12.999603	-0.057954	4.816015
284.295810	7999.809525	13.004608	-0.057953	4.816004
284.071004	7999.946474	13.009613	-0.057911	4.816045
284.330106	7999.747109	13.014618	-0.057959	4.815985
284.215865	7999.911704	13.019623	-0.057938	4.816034
284.132954	7999.867463	13.024627	-0.057922	4.816021
284.424844	7999.843909	13.029632	-0.057977	4.816013
284.212503	7999.832577	13.034637	-0.057937	4.816011
284.160520	7999.836975	13.039642	-0.057928	4.816012
284.304683	7999.901555	13.044647	-0.057954	4.816030
284.261180	7999.833455	13.049651	-0.057946	4.816011
284.442897	7999.872007	13.054656	-0.057980	4.816021
284.474725	7999.883267	13.059661	-0.057986	4.816024
284.280785	7999.801754	13.064666	-0.057950	4.816001
284.081775	7999.881478	13.069671	-0.057913	4.816026
284.352366	7999.805186	13.074675	-0.057963	4.816002
284.446202	7999.840007	13.079680	-0.057981	4.816012
284.332252	7999.891358	13.084685	-0.057959	4.816027
284.183150	7999.806386	13.089690	-0.057932	4.816003
284.281110	7999.853034	13.094695	-0.057950	4.816016
284.336682	7999.868998	13.099699	-0.057960	4.816021
284.355546	7999.819124	13.104704	-0.057964	4.816006
284.272150	7999.988553	13.109709	-0.057948	4.816056
284.288903	7999.808296	13.114714	-0.057951	4.816003
284.164632	7999.829545	13.119719	-0.057928	4.816010
284.243620	7999.787172	13.124723	-0.057943	4.815997
284.397502	7999.904280	13.129728	-0.057971	4.816031
284.458730	7999.816712	13.134733	-0.057983	4.816005
284.379637	7999.894337	13.139738	-0.057968	4.816028
284.326138	7999.830330	13.144743	-0.057958	4.816010
284.248669	7999.878069	13.149747	-0.057944	4.816024
284.217621	7999.829427	13.154752	-0.057938	4.816010
284.195236	7999.910217	13.159757	-0.057934	4.816034
284.256190	7999.758541	13.164762	-0.057945	4.815989
284.148020	7999.917904	13.169767	-0.057925	4.816036
284.090999	7999.789730	13.174771	-0.057914	4.815999
284.348631	7999.898035	13.179776	-0.057962	4.816029
284.327028	7999.897642	13.184781	-0.057958	4.816029
284.334186	7999.809093	13.189786	-0.057959	4.816003
284.212115	7999.860297	13.194791	-0.057937	4.816019
284.321713	7999.852668	13.199795	-0.057957	4.816016
284.211903	7999.791913	13.204800	-0.057937	4.815999
284.165354	7999.890428	13.209805	-0.057928	4.816028
284.509075	7999.878498	13.214810	-0.057992	4.816023
284.551269	7999.884604	13.219815	-0.058000	4.816024
284.331208	7999.773771	13.224819	-0.057959	4.815993
284.682335	7999.913689	13.229824	-0.058024	4.816032
284.492835	7999.858966	13.234829	-0.057989	4.816017
284.462894	7999.808207	13.239834	-0.057983	4.816002
284.550064	7999.928379	13.244839	-0.057999	4.816037
284.683175	7999.842115	13.249843	-0.058024	4.816011
284.552138	7999.798068	13.254848	-0.058000	4.815999
284.418623	7999.795645	13.259853	-0.057975	4.815999
284.424452	7999.832074	13.264858	-0.057976	4.816010
284.232628	7999.909791	13.269863	-0.057940	4.816033
284.409371	7999.857439	13.274867	-0.057973	4.816017
284.639515	7999.795372	13.279872	-0.058016	4.815998
284.566039	7999.854936	13.284877	-0.058002	4.816015
284.608207	7999.868520	13.289882	-0.058010	4.816019
284.480373	7999.859789	13.294887	-0.057986	4.816017
284.793272	7999.836617	13.299891	-0.058045	4.816009
284.684981	7999.813283	13.304896	-0.058024	4.816003
284.585373	7999.861689	13.309901	-0.058006	4.816017
284.672801	7999.803443	13.314906	-0.058022	4.816000
284.691964	7999.967255	13.319911	-0.058026	4.816048
284.403084	7999.795342	13.324915	-0.057972	4.815999
284.623580	7999.854897	13.329920	-0.058013	4.816015
284.596825	7999.897146	13.334925	-0.058008	4.816028
284.671936	7999.772436	13.339930	-0.058022	4.815991
284.523763	7999.901160	13.344935	-0.057994	4.816029
284.556365	7999.900681	13.349939	-0.058000	4.816029
284.651970	7999.848994	13.354944	-0.058018	4.816013
284.482151	7999.889716	13.359949	-0.057986	4.816026
284.547970	7999.777658	13.364954	-0.057999	4.815993
284.636076	7999.892505	13.369959	-0.058015	4.816026
284.485301	7999.858785	13.374963	-0.057987	4.816017
284.882029	7999.822175	13.379968	-0.058061	4.816004
284.753222	7999.829453	13.384973	-0.058037	4.816007
284.675368	7999.897485	13.389978	-0.058022	4.816027
284.638081	7999.849797	13.394983	-0.058015	4.816014
284.508410	7999.834623	13.399987	-0.057991	4.816010
284.494682	7999.815141	13.404992	-0.057989	4.816004
284.310158	7999.880169	13.409997	-0.057954	4.816024
284.490124	7999.895185	13.415002	-0.057988	4.816028
284.400990	7999.810231	13.420007	-0.057971	4.816003
284.374059	7999.827904	13.425011	-0.057966	4.816009
284.378739	7999.915596	13.430016	-0.057967	4.816034
284.466755	7999.913986	13.435021	-0.057983	4.816033
284.506344	7999.796110	13.440026	-0.057991	4.815999
284.451183	7999.847459	13.445031	-0.057980	4.816014
284.635655	7999.899951	13.450035	-0.058015	4.816028
284.516792	7999.858262	13.455040	-0.057993	4.816017
284.372211	7999.791534	13.460045	-0.057966	4.815998
284.516946	7999.887108	13.465050	-0.057993	4.816025
284.434324	7999.872787	13.470055	-0.057977	4.816021
284.318245	7999.829012	13.475059	-0.057955	4.816009
284.434302	7999.854621	13.480064	-0.057977	4.816016
284.380459	7999.926293	13.485069	-0.057967	4.816037
284.287209	7999.804940	13.490074	-0.057950	4.816002
284.423864	7999.896094	13.495079	-0.057975	4.816028
284.453652	7999.876333	13.500083	-0.057981	4.816022
284.525153	7999.862671	13.505088	-0.057994	4.816018
284.307767	7999.870478	13.510093	-0.057953	4.816021
284.471910	7999.825376	13.515098	-0.057984	4.816007
284.463193	7999.863679	13.520103	-0.057982	4.816019
284.326834	7999.850520	13.525107	-0.057957	4.816015
284.422600	7999.872555	13.530112	-0.057975	4.816021
284.474023	7999.944001	13.535117	-0.057984	4.816042
284.268550	7999.856937	13.540122	-0.057946	4.816018
284.255603	7999.846016	13.545127	-0.057944	4.816015
284.447575	7999.851634	13.550131	-0.057979	4.816015
284.392905	7999.897650	13.555136	-0.057969	4.816029
284.422453	7999.804165	13.560141	-0.057975	4.816001
284.253356	7999.930373	13.565146	-0.057943	4.816039
284.435930	7999.866374	13.570151	-0.057977	4.816020
284.340296	7999.834722	13.575155	-0.057959	4.816011
284.473830	7999.867058	13.580160	-0.057984	4.816020
284.283090	7999.859323	13.585165	-0.057949	4.816018
284.476903	7999.907710	13.590170	-0.057985	4.816031
284.367605	7999.820254	13.595175	-0.057964	4.816006
284.326082	7999.860098	13.600179	-0.057957	4.816018
284.643483	7999.867991	13.605184	-0.058016	4.816019
284.449469	7999.912548	13.610189	-0.057980	4.816033
284.535176	7999.859612	13.615194	-0.057995	4.816017
284.383391	7999.860063	13.620199	-0.057967	4.816018
284.413545	7999.870224	13.625203	-0.057973	4.816021
284.367647	7999.812764	13.630208	-0.057964	4.816004
284.279427	7999.938302	13.635213	-0.057948	4.816041
284.469602	7999.880851	13.640218	-0.057983	4.816024
284.398450	7999.875285	13.645223	-0.057970	4.816022
284.418037	7999.933333	13.650227	-0.057974	4.816039
284.443427	7999.875030	13.655232	-0.057978	4.816022
284.196039	7999.824600	13.660237	-0.057932	4.816009
284.380050	7999.851440	13.665242	-0.057966	4.816015
284.587351	7999.893662	13.670247	-0.058005	4.816027
284.501162	7999.917738	13.675251	-0.057989	4.816034
284.558232	7999.827958	13.680256	-0.057999	4.816008
284.431985	7999.859855	13.685261	-0.057976	4.816018
284.553892	7999.831081	13.690266	-0.057999	4.816009
284.477052	7999.878832	13.695271	-0.057984	4.816023
284.505511	7999.841953	13.700275	-0.057990	4.816012
284.662862	7999.933483	13.705280	-0.058019	4.816038
284.432146	7999.910065	13.710285	-0.057976	4.816032
284.360516	7999.906627	13.715290	-0.057963	4.816032
284.497792	7999.970015	13.720295	-0.057988	4.816049
284.441992	7999.874981	13.725299	-0.057978	4.816022
284.570698	7999.894409	13.730304	-0.058002	4.816027
284.403603	7999.897786	13.735309	-0.057971	4.816029
284.625570	7999.888991	13.740314	-0.058012	4.816025
284.413188	7999.911846	13.745319	-0.057972	4.816033
284.396106	7999.892304	13.750323	-0.057969	4.816027
284.679523	7999.826929	13.755328	-0.058022	4.816007
284.391545	7999.868713	13.760333	-0.057968	4.816020
284.354988	7999.941768	13.765338	-0.057961	4.816042
284.556892	7999.931540	13.770343	-0.057999	4.816038
284.528527	7999.917134	13.775347	-0.057994	4.816034
284.436729	7999.912262	13.780352	-0.057977	4.816033
284.441454	7999.889910	13.785357	-0.057977	4.816026
284.566126	7999.856913	13.790362	-0.058001	4.816016
284.394473	7999.897602	13.795367	-0.057969	4.816029
284.151505	7999.886782	13.800371	-0.057923	4.816027
284.452140	7999.939244	13.805376	-0.057979	4.816041
284.428576	7999.840522	13.810381	-0.057975	4.816012
284.414893	7999.897966	13.815386	-0.057972	4.816029
284.470638	7999.842350	13.820391	-0.057983	4.816012
284.329616	7999.888937	13.825395	-0.057956	4.816027
284.436347	7999.869503	13.830400	-0.057976	4.816020
284.331383	7999.898581	13.835405	-0.057957	4.816030
284.295455	7999.956690	13.840410	-0.057950	4.816047
284.297085	7999.965265	13.845415	-0.057950	4.816049
283.983708	7999.921116	13.850419	-0.057892	4.816038
284.186850	7999.953646	13.855424	-0.057930	4.816046
284.235406	7999.878669	13.860429	-0.057939	4.816024
284.315136	7999.894003	13.865434	-0.057954	4.816028
284.421804	7999.907689	13.870439	-0.057974	4.816032
284.552134	7999.859837	13.875443	-0.057998	4.816017
284.472854	7999.916091	13.880448	-0.057983	4.816034
284.448209	7999.909231	13.885453	-0.057978	4.816032
284.566471	7999.866502	13.890458	-0.058000	4.816019
284.541081	7999.870314	13.895463	-0.057996	4.816020
284.646816	7999.805989	13.900467	-0.058015	4.816001
284.633391	7999.879464	13.905472	-0.058013	4.816022
284.509293	7999.956273	13.910477	-0.057990	4.816045
284.348847	7999.848658	13.915482	-0.057960	4.816015
284.291700	7999.891424	13.920487	-0.057949	4.816028
284.414763	7999.854124	13.925491	-0.057972	4.816016
284.503620	7999.873897	13.930496	-0.057989	4.816021
284.556020	7999.928266	13.935501	-0.057998	4.816037
284.593090	7999.811412	13.940506	-0.058005	4.816003
284.784193	7999.840519	13.945511	-0.058041	4.816010
284.716575	7999.910874	13.950515	-0.058028	4.816031
284.594474	7999.865921	13.955520	-0.058005	4.816019
284.608563	7999.848012	13.960525	-0.058008	4.816013
284.464727	7999.845401	13.965530	-0.057981	4.816013
284.446571	7999.900627	13.970535	-0.057978	4.816030
284.460734	7999.883788	13.975539	-0.057980	4.816025
284.606184	7999.842621	13.980544	-0.058007	4.816012
284.599278	7999.954676	13.985549	-0.058006	4.816045
284.650435	7999.832736	13.990554	-0.058016	4.816009
284.649494	7999.894685	13.995559	-0.058015	4.816027
284.311664	7999.808425	14.000563	-0.057953	4.816003
284.511652	7999.866539	14.005568	-0.057990	4.816019
284.527144	7999.844382	14.010573	-0.057993	4.816013
284.612716	7999.874780	14.015578	-0.058009	4.816021
284.584718	7999.882818	14.020583	-0.058003	4.816024
284.632645	7999.905054	14.025587	-0.058012	4.816030
284.753720	7999.874128	14.030592	-0.058035	4.816020
284.468171	7999.835826	14.035597	-0.057982	4.816010
284.510156	7999.886801	14.040602	-0.057989	4.816025
284.586346	7999.925575	14.045607	-0.058004	4.816036
284.469896	7999.845468	14.050611	-0.057982	4.816013
284.535289	7999.900073	14.055616	-0.057994	4.816029
284.543371	7999.854276	14.060621	-0.057995	4.816015
284.367309	7999.859628	14.065626	-0.057963	4.816018
284.524260	7999.885979	14.070631	-0.057992	4.816025
284.463923	7999.851762	14.075635	-0.057981	4.816015
284.561123	7999.875960	14.080640	-0.057999	4.816022
284.528937	7999.867896	14.085645	-0.057993	4.816020
284.481662	7999.874515	14.090650	-0.057984	4.816022
284.585983	7999.899911	14.095655	-0.058003	4.816029
284.395288	7999.849441	14.100659	-0.057968	4.816015
284.545353	7999.904513	14.105664	-0.057996	4.816030
284.591255	7999.891455	14.110669	-0.058004	4.816026
284.531877	7999.912812	14.115674	-0.057993	4.816033
284.681193	7999.897357	14.120679	-0.058021	4.816027
284.666933	7999.812693	14.125683	-0.058018	4.816003
284.814190	7999.928614	14.130688	-0.058046	4.816036
284.562368	7999.842845	14.135693	-0.057999	4.816012
284.445566	7999.833245	14.140698	-0.057977	4.816010
284.632093	7999.919963	14.145703	-0.058012	4.816034
284.506946	7999.772389	14.150707	-0.057988	4.815992
284.434148	7999.840512	14.155712	-0.057975	4.816012
284.523511	7999.947904	14.160717	-0.057992	4.816043
284.577534	7999.800374	14.165722	-0.058001	4.816000
284.488632	7999.858590	14.170727	-0.057985	4.816017
284.584253	7999.914812	14.175731	-0.058003	4.816033
284.564274	7999.869575	14.180736	-0.057999	4.816020
284.499144	7999.850229	14.185741	-0.057987	4.816015
284.704401	7999.832583	14.190746	-0.058025	4.816008
284.745173	7999.900630	14.195751	-0.058033	4.816028
284.784807	7999.859680	14.200755	-0.058040	4.816016
284.760663	7999.926550	14.205760	-0.058036	4.816035
284.742945	7999.841823	14.210765	-0.058032	4.816011
284.536787	7999.867997	14.215770	-0.057994	4.816020
284.667073	7999.915232	14.220775	-0.058018	4.816033
284.558591	7999.864115	14.225779	-0.057998	4.816018
284.695797	7999.947802	14.230784	-0.058023	4.816042
284.527399	7999.926582	14.235789	-0.057992	4.816037
284.514251	7999.950915	14.240794	-0.057990	4.816044
284.704048	7999.926578	14.245799	-0.058025	4.816036
284.642184	7999.572884	14.250803	-0.058013	4.815933

284.766520	7996.417285	14.255808	-0.058034	4.815010
284.866865	7990.782180	14.260813	-0.058049	4.813362
284.782408	7984.008901	14.265818	-0.058029	4.811382
284.724418	7976.694783	14.270823	-0.058013	4.809242
284.490203	7969.033233	14.275827	-0.057965	4.807001
284.459436	7961.224296	14.280832	-0.057954	4.804714
284.354923	7953.377358	14.285837	-0.057929	4.802416
284.266251	7945.383282	14.290842	-0.057908	4.800073
284.458322	7937.508507	14.295847	-0.057938	4.797763
284.351657	7929.408089	14.300851	-0.057913	4.795387
284.264481	7921.405621	14.305856	-0.057892	4.793038
284.320958	7913.386040	14.310861	-0.057897	4.790683
284.089302	7905.420003	14.315866	-0.057849	4.788343
284.211181	7897.405090	14.320871	-0.057866	4.785986
283.811320	7889.427417	14.325875	-0.057786	4.783642
283.971448	7881.449628	14.330880	-0.057811	4.781293
283.757256	7873.419184	14.335885	-0.057766	4.778930
283.791539	7865.393317	14.340890	-0.057767	4.776566
283.862291	7857.419613	14.345895	-0.057775	4.774215
283.716059	7849.343998	14.350899	-0.057742	4.771835
283.866374	7841.385686	14.355904	-0.057765	4.769486
283.893895	7833.382986	14.360909	-0.057765	4.767124
283.788121	7825.334837	14.365914	-0.057740	4.764748
283.696685	7817.464207	14.370919	-0.057718	4.762423
283.508764	7809.368081	14.375923	-0.057678	4.760031
283.656383	7801.416713	14.380928	-0.057700	4.757679
283.652156	7793.390234	14.385933	-0.057694	4.755304
283.472299	7785.325445	14.390938	-0.057655	4.752917
283.565698	7777.326217	14.395943	-0.057667	4.750547
283.549072	7769.331682	14.400947	-0.057659	4.748178
283.515667	7761.348316	14.405952	-0.057648	4.745812
283.397850	7753.327945	14.410957	-0.057620	4.743433
283.435393	7745.358728	14.415962	-0.057622	4.741068
283.369288	7737.376498	14.420967	-0.057605	4.738698
283.200730	7729.317265	14.425971	-0.057568	4.736304
283.299110	7721.376519	14.430976	-0.057581	4.733944
283.239368	7713.313042	14.435981	-0.057565	4.731546
283.082748	7705.345988	14.440986	-0.057530	4.729176
282.970867	7697.343634	14.445991	-0.057504	4.726794
283.009448	7689.272548	14.450995	-0.057506	4.724390
283.034059	7681.367773	14.456000	-0.057506	4.722035
282.953858	7673.296275	14.461005	-0.057485	4.719629
282.932758	7665.374970	14.466010	-0.057476	4.717266
282.881387	7657.360089	14.471015	-0.057461	4.714874
282.802520	7649.259142	14.476019	-0.057442	4.712456
282.834143	7641.289849	14.481024	-0.057442	4.710075
282.765376	7633.357077	14.486029	-0.057424	4.707704
282.588771	7625.261413	14.491034	-0.057386	4.705283
282.548217	7617.381913	14.496039	-0.057373	4.702926
282.423765	7609.296091	14.501043	-0.057345	4.700506
282.698593	7601.339776	14.506048	-0.057391	4.698122
282.515844	7593.337813	14.511053	-0.057352	4.695725
282.429314	7585.315802	14.516058	-0.057330	4.693320
282.482364	7577.257415	14.521063	-0.057335	4.690902
282.233698	7569.300709	14.526067	-0.057283	4.688515
282.205570	7561.321734	14.531072	-0.057273	4.686119
282.099668	7553.302661	14.536077	-0.057248	4.683710
282.219525	7545.303890	14.541082	-0.057265	4.681306
282.014613	7537.301780	14.546087	-0.057222	4.678900
282.134168	7529.314329	14.551091	-0.057239	4.676496
282.155503	7521.245299	14.556096	-0.057237	4.674067
281.772567	7513.192442	14.561101	-0.057161	4.671642
281.824952	7505.211810	14.566106	-0.057165	4.669237
281.943128	7497.229453	14.571111	-0.057182	4.666830
281.716602	7489.174732	14.576115	-0.057135	4.664400
281.762720	7481.270565	14.581120	-0.057138	4.662014
281.835072	7473.228980	14.586125	-0.057146	4.659586
281.717815	7465.250517	14.591130	-0.057119	4.657175
281.660210	7457.265174	14.596135	-0.057103	4.654761
281.541343	7449.252759	14.601139	-0.057076	4.652338
281.641239	7441.208427	14.606144	-0.057089	4.649903
281.671412	7433.233953	14.611149	-0.057090	4.647489
281.616436	7425.208663	14.616154	-0.057074	4.645058
281.437732	7417.285978	14.621159	-0.057036	4.642657
281.366749	7409.185698	14.626163	-0.057017	4.640200
281.472545	7401.304331	14.631168	-0.057032	4.637809
281.316943	7393.241061	14.636173	-0.056998	4.635361
281.280362	7385.214347	14.641178	-0.056985	4.632923
281.370296	7377.216901	14.646183	-0.056997	4.630493
281.315426	7369.176012	14.651187	-0.056981	4.628048
281.352921	7361.198117	14.656192	-0.056983	4.625621
281.053659	7353.251299	14.661197	-0.056922	4.623202
280.988161	7345.178082	14.666202	-0.056905	4.620744
281.342590	7337.233964	14.671207	-0.056966	4.618323
281.064959	7329.177077	14.676211	-0.056909	4.615867
280.954034	7321.170904	14.681216	-0.056883	4.613425
280.793349	7313.197589	14.686221	-0.056848	4.610991
280.749516	7305.162251	14.691226	-0.056834	4.608538
280.746281	7297.174165	14.696231	-0.056828	4.606097
280.724032	7289.169887	14.701235	-0.056819	4.603651
280.786095	7281.215855	14.706240	-0.056825	4.601218
280.586202	7273.194511	14.711245	-0.056783	4.598763
280.402691	7265.185695	14.716250	-0.056744	4.596311
280.553023	7257.170026	14.721255	-0.056766	4.593856
280.305378	7249.101643	14.726259	-0.056715	4.591383
280.243535	7241.166900	14.731264	-0.056698	4.588950
280.434325	7233.126386	14.736269	-0.056728	4.586483
280.361135	7225.140158	14.741274	-0.056710	4.584031
280.354516	7217.183578	14.746279	-0.056703	4.581587
280.163393	7209.156315	14.751283	-0.056662	4.579120
280.212382	7201.187946	14.756288	-0.056666	4.576670
280.134147	7193.145916	14.761293	-0.056646	4.574196
279.895927	7185.131878	14.766298	-0.056597	4.571729
280.132338	7177.133502	14.771303	-0.056636	4.569265
280.022709	7169.101610	14.776307	-0.056610	4.566790
280.115474	7161.133375	14.781312	-0.056622	4.564334
279.924763	7153.183275	14.786317	-0.056581	4.561881
279.712489	7145.158718	14.791322	-0.056537	4.559404
279.841870	7137.208360	14.796327	-0.056555	4.556949
279.743163	7129.124570	14.801331	-0.056532	4.554451
279.883927	7121.118166	14.806336	-0.056553	4.551976
279.580618	7113.077270	14.811341	-0.056491	4.549488
279.511327	7105.129784	14.816346	-0.056473	4.547028
279.623953	7097.101259	14.821351	-0.056489	4.544542
279.512460	7089.167666	14.826355	-0.056463	4.542084
279.487412	7081.139381	14.831360	-0.056453	4.539595
279.588117	7073.163253	14.836365	-0.056466	4.537121
279.474782	7065.142162	14.841370	-0.056440	4.534632
279.399608	7057.131374	14.846375	-0.056421	4.532144
279.270597	7049.068034	14.851379	-0.056391	4.529639
279.238355	7041.134208	14.856384	-0.056380	4.527172
279.286694	7033.111965	14.861389	-0.056384	4.524677
279.035675	7025.169046	14.866394	-0.056332	4.522205
279.134985	7017.142322	14.871399	-0.056345	4.519706
279.007628	7009.160449	14.876403	-0.056316	4.517219
278.922090	7001.116687	14.881408	-0.056295	4.514711
278.794544	6993.001654	14.886413	-0.056266	4.512180
278.860996	6984.998960	14.891418	-0.056273	4.509683
278.971483	6977.072349	14.896423	-0.056289	4.507208
278.802435	6969.003168	14.901427	-0.056252	4.504687
278.922058	6961.116216	14.906432	-0.056269	4.502221
278.750766	6953.067057	14.911437	-0.056232	4.499704
278.595961	6945.105135	14.916442	-0.056198	4.497212
278.735562	6937.071631	14.921447	-0.056219	4.494696
278.592863	6929.086680	14.926451	-0.056187	4.492194
278.526971	6921.058815	14.931456	-0.056169	4.489678
278.421279	6913.084582	14.936461	-0.056144	4.487176
278.414026	6905.024488	14.941466	-0.056138	4.484647
278.552345	6897.117767	14.946471	-0.056158	4.482165
278.363778	6889.041484	14.951475	-0.056118	4.479627
278.450487	6881.127188	14.956480	-0.056129	4.477139
278.202412	6873.061630	14.961485	-0.056078	4.474602
278.080946	6865.013428	14.966490	-0.056050	4.472068
278.286667	6857.040986	14.971495	-0.056083	4.469559
278.115698	6849.004386	14.976499	-0.056046	4.467026
278.041874	6841.012026	14.981504	-0.056027	4.464506
278.007516	6833.046565	14.986509	-0.056015	4.461994
278.039996	6825.011725	14.991514	-0.056016	4.459458
278.243078	6817.097237	14.996519	-0.056049	4.456960
277.957838	6809.051196	15.001523	-0.055990	4.454416
278.162123	6801.062670	15.006528	-0.056023	4.451892
278.041347	6793.041830	15.011533	-0.055995	4.449354
277.995577	6785.020814	15.016538	-0.055981	4.446815
277.926204	6777.044105	15.021543	-0.055963	4.444289
277.774920	6769.034528	15.026547	-0.055930	4.441750
277.567648	6761.047997	15.031552	-0.055886	4.439218
277.657081	6753.029010	15.036557	-0.055898	4.436674
277.717033	6745.012014	15.041562	-0.055903	4.434130
277.485619	6736.976770	15.046567	-0.055855	4.431577
277.077899	6728.969157	15.051571	-0.055774	4.429030
277.075737	6720.959046	15.056576	-0.055768	4.426483
277.231522	6713.002470	15.061581	-0.055792	4.423953
277.247215	6705.003258	15.066586	-0.055790	4.421406
277.105143	6697.003955	15.071591	-0.055758	4.418858
277.239071	6688.959474	15.076595	-0.055778	4.416295
277.087696	6680.983336	15.081600	-0.055744	4.413751
277.058255	6672.982737	15.086605	-0.055734	4.411198
277.005013	6664.978335	15.091610	-0.055719	4.408642
276.907021	6656.959719	15.096615	-0.055695	4.406080
276.702829	6648.991333	15.101619	-0.055652	4.403532
276.840601	6641.031286	15.106624	-0.055672	4.400987
276.732156	6633.050289	15.111629	-0.055647	4.398433
276.692776	6625.007604	15.116634	-0.055634	4.395858
276.618624	6616.981890	15.121639	-0.055615	4.393286
276.772907	6608.930036	15.126643	-0.055639	4.390706
276.887956	6601.009989	15.131648	-0.055655	4.388166
276.580580	6592.971024	15.136653	-0.055592	4.385584
276.409196	6585.023138	15.141658	-0.055555	4.383031
276.494828	6576.997011	15.146663	-0.055566	4.380453
276.427828	6569.023775	15.151667	-0.055548	4.377889
276.372602	6561.017206	15.156672	-0.055533	4.375313
276.488623	6553.006621	15.161677	-0.055549	4.372735
276.276668	6544.995765	15.166682	-0.055504	4.370154
276.300927	6537.019479	15.171687	-0.055504	4.367583
276.253446	6528.948499	15.176691	-0.055490	4.364981
276.245312	6521.035459	15.181696	-0.055483	4.362427
276.098478	6512.989403	15.186701	-0.055450	4.359829
276.110155	6505.022594	15.191706	-0.055447	4.357256
276.361510	6497.021285	15.196711	-0.055489	4.354671
276.119601	6488.870795	15.201715	-0.055439	4.352033
275.904811	6480.876255	15.206720	-0.055393	4.349445
275.790094	6472.935738	15.211725	-0.055367	4.346873
275.622869	6464.959568	15.216730	-0.055330	4.344288
275.889793	6457.008621	15.221735	-0.055375	4.341712
275.601697	6448.932772	15.226739	-0.055316	4.339090
275.715868	6440.986607	15.231744	-0.055332	4.336512
275.566417	6432.977400	15.236749	-0.055299	4.333910
275.628084	6424.941891	15.241754	-0.055305	4.331299
275.468078	6416.991584	15.246759	-0.055270	4.328712
275.432833	6408.935122	15.251763	-0.055258	4.326091
275.363568	6400.980144	15.256768	-0.055240	4.323500
275.567157	6393.003134	15.261773	-0.055273	4.320903
275.260266	6384.967988	15.266778	-0.055211	4.318282
275.316080	6376.973120	15.271783	-0.055216	4.315675
275.449703	6368.925914	15.276787	-0.055235	4.313050
275.381864	6360.900394	15.281792	-0.055218	4.310428
275.123578	6352.960411	15.286797	-0.055164	4.307832
275.012512	6344.912269	15.291802	-0.055138	4.305200
275.140889	6336.986790	15.296807	-0.055157	4.302608
275.078961	6328.934014	15.301811	-0.055140	4.299971
274.975650	6320.968148	15.306816	-0.055116	4.297362
274.957743	6312.935688	15.311821	-0.055107	4.294729
274.848871	6304.904573	15.316826	-0.055082	4.292094
275.087850	6296.891210	15.321831	-0.055121	4.289466
274.845655	6288.927312	15.326835	-0.055071	4.286849
274.878703	6280.924775	15.331840	-0.055072	4.284220
274.798829	6273.014349	15.336845	-0.055051	4.281619
274.748101	6264.942981	15.341850	-0.055037	4.278964
274.789314	6256.973017	15.346855	-0.055039	4.276340
274.608476	6248.948963	15.351859	-0.055000	4.273696
274.490034	6240.845076	15.356864	-0.054973	4.271024
274.537493	6232.894536	15.361869	-0.054977	4.268403
274.482580	6224.858759	15.366874	-0.054961	4.265751
274.397723	6216.942198	15.371879	-0.054940	4.263136
274.046767	6208.899429	15.376883	-0.054870	4.260476
274.221094	6200.921922	15.381888	-0.054897	4.257840
274.130588	6192.912776	15.386893	-0.054875	4.255189
274.117056	6184.902877	15.391898	-0.054867	4.252538
274.118833	6176.912660	15.396903	-0.054862	4.249891
274.051481	6168.942448	15.401907	-0.054844	4.247249
273.929004	6160.876127	15.406912	-0.054816	4.244573
274.108241	6152.977988	15.411917	-0.054844	4.241954
274.122149	6144.927486	15.416922	-0.054842	4.239281
274.129829	6136.987438	15.421927	-0.054838	4.236643
273.850521	6128.930700	15.426931	-0.054781	4.233961
273.961267	6120.892758	15.431936	-0.054796	4.231288
273.939130	6112.893572	15.436941	-0.054787	4.228625
273.829298	6104.859747	15.441946	-0.054761	4.225948
273.703822	6096.961662	15.446951	-0.054732	4.223314
273.536577	6088.946232	15.451955	-0.054696	4.220640
273.638005	6080.980614	15.456960	-0.054710	4.217982
273.631048	6072.970779	15.461965	-0.054703	4.215307
273.436713	6064.925729	15.466970	-0.054662	4.212617
273.413349	6056.955565	15.471975	-0.054652	4.209952
273.223975	6048.937531	15.476979	-0.054612	4.207267
273.356903	6040.924451	15.481984	-0.054631	4.204586
273.501031	6032.989698	15.486989	-0.054653	4.201929
273.111967	6024.951198	15.491994	-0.054575	4.199230
273.402526	6016.983982	15.496999	-0.054624	4.196560
273.127029	6008.893924	15.502003	-0.054568	4.193842
273.035692	6000.830532	15.507008	-0.054545	4.191133
273.025368	5992.846972	15.512013	-0.054538	4.188449
272.813412	5984.873875	15.517018	-0.054493	4.185766
272.931709	5976.968929	15.522023	-0.054510	4.183107
272.802290	5968.909933	15.527027	-0.054481	4.180392
272.890087	5960.946611	15.532032	-0.054492	4.177709
272.817387	5952.932396	15.537037	-0.054473	4.175006
272.527019	5944.922057	15.542042	-0.054414	4.172300
272.530601	5936.925131	15.547047	-0.054409	4.169600
272.510392	5928.891667	15.552051	-0.054400	4.166886
272.550036	5920.898429	15.557056	-0.054403	4.164184
272.411265	5912.943904	15.562061	-0.054372	4.161492
272.568840	5904.924877	15.567066	-0.054396	4.158779
272.432726	5896.929993	15.572071	-0.054365	4.156070
272.430497	5888.909211	15.577075	-0.054359	4.153351
272.412045	5880.860188	15.582080	-0.054351	4.150621
272.420960	5872.896475	15.587085	-0.054347	4.147918
272.269530	5864.883672	15.592090	-0.054314	4.145195
272.376658	5856.936244	15.597095	-0.054328	4.142495
272.287378	5848.853869	15.602099	-0.054307	4.139746
272.166782	5840.923820	15.607104	-0.054279	4.137046
272.000888	5832.919006	15.612109	-0.054243	4.134318
271.909131	5824.848264	15.617114	-0.054220	4.131567
272.044756	5816.910417	15.622119	-0.054240	4.128862
271.940313	5808.908459	15.627123	-0.054216	4.126131
271.893288	5800.931748	15.632128	-0.054202	4.123407
271.912129	5792.924180	15.637133	-0.054200	4.120671
271.604271	5784.925456	15.642138	-0.054138	4.117933
271.714116	5776.928040	15.647143	-0.054153	4.115199
271.716539	5768.843166	15.652147	-0.054148	4.112431
271.787269	5760.853265	15.657152	-0.054156	4.109695
271.387055	5752.931482	15.662157	-0.054076	4.106974
271.490055	5744.890999	15.667162	-0.054090	4.104218
271.442934	5736.934194	15.672167	-0.054076	4.101486
271.316402	5728.911172	15.677171	-0.054047	4.098728
271.246960	5720.916892	15.682176	-0.054029	4.095980
271.558787	5712.906382	15.687181	-0.054082	4.093229
271.505370	5704.869636	15.692186	-0.054067	4.090462
271.306807	5696.947192	15.697191	-0.054025	4.087731
271.264671	5688.898268	15.702195	-0.054012	4.084956
271.198735	5680.965254	15.707200	-0.053994	4.082220
271.217984	5672.938439	15.712205	-0.053992	4.079450
271.179841	5664.976240	15.717210	-0.053980	4.076700
271.051942	5656.947083	15.722215	-0.053951	4.073923
270.956730	5648.897809	15.727219	-0.053928	4.071138
271.044798	5640.924420	15.732224	-0.053939	4.068380
271.006168	5632.914567	15.737229	-0.053927	4.065606
271.054041	5624.935578	15.742234	-0.053931	4.062842
271.032232	5616.954897	15.747239	-0.053921	4.060074
270.847728	5608.975428	15.752243	-0.053882	4.057303
270.979490	5600.928488	15.757248	-0.053901	4.054511
270.880973	5592.962865	15.762253	-0.053877	4.051741
270.765325	5584.906499	15.767258	-0.053851	4.048938
270.811598	5576.950480	15.772263	-0.053854	4.046171
270.505121	5568.961548	15.777267	-0.053792	4.043385
270.547845	5560.934239	15.782272	-0.053794	4.040588
270.683802	5552.983786	15.787277	-0.053815	4.037818
270.496471	5544.951177	15.792282	-0.053774	4.035013
270.320269	5536.867462	15.797287	-0.053736	4.032188
270.035989	5528.869084	15.802291	-0.053678	4.029389
270.180901	5520.875157	15.807296	-0.053700	4.026596
270.130772	5512.909299	15.812301	-0.053685	4.023808
269.994281	5504.894748	15.817306	-0.053655	4.021000
270.233396	5496.924944	15.822311	-0.053694	4.018211
270.172275	5488.911234	15.827315	-0.053677	4.015400
270.211203	5480.913061	15.832320	-0.053679	4.012594
270.236772	5472.891723	15.837325	-0.053679	4.009778
270.052270	5464.896755	15.842330	-0.053639	4.006966
269.966391	5456.912914	15.847335	-0.053618	4.004158
269.998631	5448.954338	15.852339	-0.053619	4.001358
269.977822	5440.942521	15.857344	-0.053610	3.998536
269.762169	5432.947709	15.862349	-0.053564	3.995716
269.566365	5424.895796	15.867354	-0.053523	3.992874
269.812559	5416.894415	15.872359	-0.053563	3.990054
269.908949	5408.893863	15.877363	-0.053576	3.987231
269.743551	5400.919639	15.882368	-0.053540	3.984410
269.752188	5392.952927	15.887373	-0.053536	3.981593
269.670915	5384.918354	15.892378	-0.053516	3.978749
269.440101	5376.966056	15.897383	-0.053468	3.975929
269.336471	5368.919408	15.902387	-0.053443	3.973076
269.254726	5360.944463	15.907392	-0.053423	3.970246
269.328371	5352.945157	15.912397	-0.053431	3.967409
269.199161	5344.931140	15.917402	-0.053402	3.964561
269.223071	5337.009729	15.922407	-0.053401	3.961746
269.148298	5328.981878	15.927411	-0.053382	3.958890
269.156232	5320.998919	15.932416	-0.053378	3.956049
269.144646	5312.956905	15.937421	-0.053371	3.953184
268.864637	5304.913386	15.942426	-0.053314	3.950312
268.969316	5296.954556	15.947431	-0.053328	3.947476
268.990360	5288.916245	15.952435	-0.053327	3.944607
268.822334	5280.982019	15.957440	-0.053290	3.941770
268.725128	5272.993404	15.962445	-0.053267	3.938912
268.680160	5264.982792	15.967450	-0.053253	3.936046
268.802726	5256.996016	15.972455	-0.053271	3.933189
268.652463	5248.986556	15.977459	-0.053238	3.930317
268.454010	5241.017603	15.982464	-0.053195	3.927457
268.693778	5232.965912	15.987469	-0.053235	3.924573
268.501885	5225.009260	15.992474	-0.053194	3.921712
268.556068	5217.008896	15.997479	-0.053199	3.918839
268.457245	5209.033318	16.002483	-0.053175	3.915970
268.481504	5201.004549	16.007488	-0.053174	3.913081
268.277844	5192.974122	16.012493	-0.053131	3.910186
268.291986	5184.991549	16.017498	-0.053129	3.907309
268.368640	5176.985719	16.022503	-0.053138	3.904424
268.323911	5169.026560	16.027507	-0.053124	3.901551
268.131764	5161.015159	16.032512	-0.053083	3.898654
268.170629	5153.012615	16.037517	-0.053085	3.895762
267.930723	5145.023474	16.042522	-0.053035	3.892868
267.948262	5136.990848	16.047527	-0.053033	3.889961
267.870326	5128.990725	16.052531	-0.053013	3.887061
267.987633	5120.979543	16.057536	-0.053030	3.884159
268.018972	5113.031280	16.062541	-0.053031	3.881277
267.847081	5105.011052	16.067546	-0.052993	3.878362
268.051892	5097.021738	16.072551	-0.053026	3.875463
267.659025	5088.804734	16.077555	-0.052948	3.872468
267.578917	5080.834087	16.082560	-0.052928	3.869566
267.572207	5072.933251	16.087565	-0.052921	3.866688
267.595690	5064.939062	16.092570	-0.052920	3.863776
267.572062	5056.991937	16.097575	-0.052911	3.860877
267.359911	5048.999394	16.102579	-0.052866	3.857956
267.354767	5040.988133	16.107584	-0.052860	3.855029
267.297864	5032.996873	16.112589	-0.052844	3.852107
267.157558	5024.971891	16.117594	-0.052813	3.849169
267.447817	5016.985823	16.122599	-0.052862	3.846251
267.172393	5009.009482	16.127603	-0.052805	3.843323
266.956288	5001.024161	16.132608	-0.052760	3.840391
267.134126	4993.061540	16.137613	-0.052788	3.837473
267.105181	4985.031387	16.142618	-0.052777	3.834523
267.172907	4977.024131	16.147623	-0.052784	3.831582
267.113617	4969.033490	16.152627	-0.052768	3.828642
266.947760	4961.055839	16.157632	-0.052732	3.825702
267.023988	4953.089423	16.162637	-0.052741	3.822770
266.749480	4945.076082	16.167642	-0.052685	3.819810
266.713430	4937.114788	16.172647	-0.052673	3.816872
266.626248	4929.099155	16.177651	-0.052651	3.813911
266.564032	4921.061341	16.182656	-0.052634	3.810940
266.539547	4913.104471	16.187661	-0.052625	3.807997
266.534644	4905.061568	16.192666	-0.052618	3.805020
266.633129	4897.120971	16.197671	-0.052632	3.802082
266.705361	4889.091166	16.202675	-0.052640	3.799107
266.520451	4881.130494	16.207680	-0.052600	3.796150
266.499679	4873.070724	16.212685	-0.052591	3.793158
266.201509	4865.051167	16.217690	-0.052530	3.790172
266.246246	4857.077571	16.222695	-0.052533	3.787208
266.194211	4849.087376	16.227699	-0.052518	3.784234
266.229056	4841.080770	16.232704	-0.052520	3.781253
266.205772	4833.109868	16.237709	-0.052510	3.778282
265.995361	4825.084405	16.242714	-0.052466	3.775284
266.061450	4817.118337	16.247719	-0.052473	3.772311
266.089871	4809.090606	16.252723	-0.052473	3.769313
265.977031	4801.085237	16.257728	-0.052447	3.766318
266.013734	4793.124005	16.262733	-0.052448	3.763339
265.687244	4785.126811	16.267738	-0.052382	3.760337
265.761767	4777.175995	16.272743	-0.052391	3.757359
265.688758	4769.115611	16.277747	-0.052372	3.754334
265.546032	4761.093444	16.282752	-0.052340	3.751320
265.569842	4753.110813	16.287757	-0.052339	3.748321
265.518638	4745.070272	16.292762	-0.052325	3.745297
265.537664	4737.159656	16.297767	-0.052323	3.742321
265.268811	4729.139675	16.302771	-0.052268	3.739294
265.472666	4721.131826	16.307776	-0.052300	3.736281
265.360358	4713.146679	16.312781	-0.052274	3.733266
265.280146	4705.115610	16.317786	-0.052254	3.730233
265.261929	4697.164061	16.322791	-0.052245	3.727228
265.259230	4689.142860	16.327795	-0.052240	3.724195
265.250938	4681.200299	16.332800	-0.052233	3.721189
265.088002	4673.218710	16.337805	-0.052197	3.718163
265.043270	4665.215639	16.342810	-0.052184	3.715128
265.011069	4657.142654	16.347815	-0.052173	3.712065
264.796954	4649.112593	16.352819	-0.052128	3.709011
264.744155	4641.146292	16.357824	-0.052112	3.705982
264.814997	4633.191742	16.362829	-0.052120	3.702959
264.751378	4625.150630	16.367834	-0.052103	3.699897
264.705110	4617.234703	16.372839	-0.052090	3.696880
264.738702	4609.189128	16.377843	-0.052091	3.693814
264.737283	4601.206476	16.382848	-0.052085	3.690768
264.728288	4593.232549	16.387853	-0.052078	3.687723
264.644675	4585.177814	16.392858	-0.052057	3.684643
264.662739	4577.279854	16.397863	-0.052056	3.681622
264.356789	4569.275125	16.402867	-0.051993	3.678550
264.275135	4561.251877	16.407872	-0.051973	3.675474
264.520207	4553.226847	16.412877	-0.052013	3.672403
264.341158	4545.200722	16.417882	-0.051975	3.669318
264.598387	4537.235340	16.422887	-0.052017	3.666265
264.364708	4529.248287	16.427891	-0.051969	3.663188
264.314038	4521.250156	16.432896	-0.051954	3.660110
264.106404	4513.291986	16.437901	-0.051910	3.657040
264.150560	4505.229758	16.442906	-0.051913	3.653934
264.272737	4497.241928	16.447911	-0.051931	3.650856
264.120593	4489.260728	16.452915	-0.051897	3.647771
263.983430	4481.236071	16.457920	-0.051866	3.644667
264.155474	4473.304635	16.462925	-0.051893	3.641604
263.797460	4465.302234	16.467930	-0.051821	3.638497
263.860145	4457.328031	16.472935	-0.051828	3.635410
263.830136	4449.250222	16.477939	-0.051817	3.632277
264.093567	4441.226786	16.482944	-0.051861	3.629171
263.909580	4433.286747	16.487949	-0.051821	3.626082
263.727174	4425.276379	16.492954	-0.051782	3.622964
263.788790	4417.330682	16.497959	-0.051788	3.619874
263.611406	4409.337831	16.502963	-0.051750	3.616757
263.498728	4401.316216	16.507968	-0.051724	3.613628
263.506438	4393.307593	16.512973	-0.051720	3.610504
263.339194	4385.314169	16.517978	-0.051684	3.607379
263.302430	4377.340146	16.522983	-0.051672	3.604263
263.120267	4369.380099	16.527987	-0.051632	3.601145
263.087387	4361.374226	16.532992	-0.051621	3.598010
263.074501	4353.389069	16.537997	-0.051613	3.594882
263.044001	4345.331742	16.543002	-0.051603	3.591721
263.210037	4337.365328	16.548007	-0.051628	3.588600
263.042752	4329.376364	16.553011	-0.051592	3.585457
262.996367	4321.388999	16.558016	-0.051578	3.582316
263.033979	4313.407389	16.563021	-0.051580	3.579176
263.035717	4305.390982	16.568026	-0.051575	3.576019
262.953335	4297.418612	16.573031	-0.051554	3.572875
262.718662	4289.393936	16.578035	-0.051505	3.569702
262.696382	4281.428256	16.583040	-0.051496	3.566556
262.693854	4273.440545	16.588045	-0.051490	3.563399
262.485037	4265.423706	16.593050	-0.051446	3.560222
262.645838	4257.493467	16.598055	-0.051471	3.557087
262.431596	4249.432313	16.603059	-0.051426	3.553886
262.357372	4241.344615	16.608064	-0.051407	3.550676
262.292290	4233.384649	16.613069	-0.051389	3.547514
262.393140	4225.374771	16.618074	-0.051403	3.544334
262.506808	4217.429939	16.623079	-0.051419	3.541178
262.393012	4209.428317	16.628083	-0.051392	3.537989
262.266739	4201.428631	16.633088	-0.051364	3.534798
262.346073	4193.413032	16.638093	-0.051373	3.531604
262.041548	4185.442815	16.643098	-0.051311	3.528414
262.211329	4177.454453	16.648103	-0.051338	3.525227
262.006035	4169.501508	16.653107	-0.051294	3.522041
261.869975	4161.498389	16.658112	-0.051264	3.518834
261.913357	4153.507737	16.663117	-0.051267	3.515634
261.792708	4145.458198	16.668122	-0.051239	3.512403
261.862917	4137.497234	16.673127	-0.051247	3.509210
261.809983	4129.457337	16.678131	-0.051232	3.505979
261.739048	4121.530261	16.683136	-0.051213	3.502789
261.649229	4113.542103	16.688141	-0.051191	3.499572
261.491739	4105.568869	16.693146	-0.051157	3.496355
261.649062	4097.569485	16.698151	-0.051181	3.493135
261.500119	4089.534588	16.703155	-0.051148	3.489888
261.512630	4081.568893	16.708160	-0.051145	3.486670
261.401252	4073.602425	16.713165	-0.051119	3.483446
261.324859	4065.618302	16.718170	-0.051100	3.480213
261.358340	4057.626897	16.723175	-0.051101	3.476977
261.398010	4049.596256	16.728179	-0.051103	3.473722
261.116774	4041.559098	16.733184	-0.051045	3.470451
261.267828	4033.591669	16.738189	-0.051068	3.467220
261.033601	4025.596752	16.743194	-0.051019	3.463962
260.959099	4017.625981	16.748199	-0.051000	3.460715
260.940973	4009.663622	16.753203	-0.050991	3.457471
260.960877	4001.629195	16.758208	-0.050990	3.454196
261.001081	3993.618353	16.763213	-0.050992	3.450928
260.880428	3985.629458	16.768218	-0.050964	3.447660
260.788373	3977.613856	16.773223	-0.050942	3.444380
260.577559	3969.688661	16.778227	-0.050898	3.441129
260.606170	3961.666490	16.783232	-0.050898	3.437844
260.491538	3953.701577	16.788237	-0.050871	3.434574
260.487342	3945.644154	16.793242	-0.050865	3.431266
260.481450	3937.666798	16.798247	-0.050859	3.427988
260.659457	3929.625995	16.803251	-0.050887	3.424687
260.544951	3921.700063	16.808256	-0.050860	3.421421
260.434265	3913.715561	16.813261	-0.050834	3.418127
260.403662	3905.687622	16.818266	-0.050823	3.414815
260.414991	3897.707893	16.823271	-0.050820	3.411521
260.364094	3889.714556	16.828275	-0.050806	3.408216
260.348085	3881.716320	16.833280	-0.050797	3.404907
260.181266	3873.781283	16.838285	-0.050761	3.401616
259.928743	3865.811409	16.843290	-0.050709	3.398304
260.002211	3857.810348	16.848295	-0.050717	3.394987
259.809633	3849.742266	16.853299	-0.050676	3.391630
259.816006	3841.726491	16.858304	-0.050672	3.388298
259.775712	3833.742749	16.863309	-0.050659	3.384975
259.705303	3825.800111	16.868314	-0.050641	3.381664
259.732687	3817.806932	16.873319	-0.050641	3.378333
259.636179	3809.820837	16.878323	-0.050618	3.374997
259.500582	3801.835528	16.883328	-0.050587	3.371656
259.514102	3793.835897	16.888333	-0.050585	3.368312
259.438180	3785.836876	16.893338	-0.050565	3.364961
259.422080	3777.894407	16.898343	-0.050557	3.361632
259.397580	3769.881666	16.903347	-0.050547	3.358271
259.194423	3761.887000	16.908352	-0.050504	3.354907
259.110484	3753.880608	16.913357	-0.050483	3.351539
259.043151	3745.867533	16.918362	-0.050466	3.348166
259.076132	3737.876925	16.923367	-0.050467	3.344803
258.924604	3729.929475	16.928371	-0.050433	3.341447
258.788114	3721.929626	16.933376	-0.050403	3.338066
259.067837	3713.907129	16.938381	-0.050449	3.334688
258.878954	3705.921439	16.943386	-0.050409	3.331305
258.820106	3697.946668	16.948391	-0.050393	3.327927
258.783545	3689.936841	16.953395	-0.050381	3.324533
258.698204	3681.986562	16.958400	-0.050360	3.321158
258.668965	3674.018188	16.963405	-0.050349	3.317774
258.469317	3666.016359	16.968410	-0.050307	3.314366
258.574986	3657.976970	16.973415	-0.050321	3.310950
258.374211	3649.997723	16.978419	-0.050278	3.307544
258.476246	3641.986171	16.983424	-0.050292	3.304133
258.468063	3634.019649	16.988429	-0.050285	3.300733
258.385168	3626.036554	16.993434	-0.050265	3.297320
258.449309	3618.065494	16.998439	-0.050272	3.293914
258.433309	3610.041992	17.003443	-0.050263	3.290478
258.145394	3602.064243	17.008448	-0.050204	3.287049
258.048385	3594.101903	17.013453	-0.050181	3.283630
257.876344	3586.087049	17.018458	-0.050144	3.280181
257.943377	3578.142723	17.023463	-0.050151	3.276769
257.860624	3570.119327	17.028467	-0.050131	3.273313
257.905235	3562.084271	17.033472	-0.050134	3.269854
257.992621	3554.126196	17.038477	-0.050145	3.266426
257.808395	3546.119354	17.043482	-0.050105	3.262962
257.750159	3538.142166	17.048487	-0.050089	3.259513
257.936418	3530.161315	17.053491	-0.050119	3.256067
257.806351	3522.175145	17.058496	-0.050089	3.252604
257.761693	3514.165994	17.063501	-0.050076	3.249130
257.589295	3506.185756	17.068506	-0.050038	3.245660
257.718199	3498.221695	17.073511	-0.050057	3.242205
257.541378	3490.225291	17.078515	-0.050019	3.238720
257.290312	3482.280975	17.083520	-0.049967	3.235251
257.480248	3474.185034	17.088525	-0.049997	3.231730
257.174458	3466.194464	17.093530	-0.049935	3.228232
257.211076	3458.205254	17.098535	-0.049936	3.224743
257.194362	3450.266022	17.103539	-0.049928	3.221271
257.126094	3442.273157	17.108544	-0.049910	3.217769
257.136461	3434.298782	17.113549	-0.049907	3.214275
257.062344	3426.255625	17.118554	-0.049888	3.210744
257.110741	3418.306504	17.123559	-0.049892	3.207255
256.986245	3410.330436	17.128563	-0.049863	3.203743
256.932940	3402.351519	17.133568	-0.049848	3.200229
256.886788	3394.409756	17.138573	-0.049834	3.196727
256.890057	3386.352508	17.143578	-0.049830	3.193173
256.805405	3378.340111	17.148583	-0.049809	3.189631
256.625238	3370.378891	17.153587	-0.049770	3.186104
256.747273	3362.371771	17.158592	-0.049787	3.182565
256.802644	3354.413651	17.163597	-0.049793	3.179041
256.578754	3346.414309	17.168602	-0.049746	3.175484
256.555673	3338.423112	17.173607	-0.049736	3.171934
256.583707	3330.408605	17.178611	-0.049736	3.168372
256.390848	3322.450950	17.183616	-0.049695	3.164822
256.451119	3314.492674	17.188621	-0.049701	3.161278
256.300681	3306.495759	17.193626	-0.049668	3.157705
256.388811	3298.482133	17.198631	-0.049679	3.154130
256.181829	3290.494954	17.203635	-0.049635	3.150550
256.193838	3282.470623	17.208640	-0.049632	3.146958
256.128566	3274.527715	17.213645	-0.049615	3.143396
255.814349	3266.534631	17.218650	-0.049551	3.139797
256.008042	3258.563139	17.223655	-0.049582	3.136225
256.016094	3250.538987	17.228659	-0.049578	3.132617
255.690865	3242.548412	17.233664	-0.049512	3.129005
255.716351	3234.595801	17.238669	-0.049512	3.125422
255.617734	3226.628548	17.243674	-0.049488	3.121823
255.801260	3218.642730	17.248679	-0.049517	3.118223
255.614640	3210.676377	17.253683	-0.049477	3.114612
255.626311	3202.636345	17.258688	-0.049474	3.110972
255.527805	3194.667575	17.263693	-0.049451	3.107355
255.472255	3186.656432	17.268698	-0.049435	3.103717
255.455028	3178.714075	17.273703	-0.049427	3.100107
255.555934	3170.740391	17.278707	-0.049440	3.096485
255.324394	3162.703707	17.283712	-0.049392	3.092814
255.476404	3154.717661	17.288717	-0.049415	3.089179
255.296140	3146.731894	17.293722	-0.049376	3.085525
255.377755	3138.775781	17.298727	-0.049386	3.081892
255.312206	3130.807010	17.303731	-0.049369	3.078243
255.232157	3122.804242	17.308736	-0.049349	3.074573
255.327771	3114.718493	17.313741	-0.049361	3.070868
255.116698	3106.755042	17.318746	-0.049317	3.067201
255.083095	3098.790680	17.323751	-0.049305	3.063537
255.066773	3090.829364	17.328755	-0.049297	3.059871
255.014636	3082.853493	17.333760	-0.049282	3.056193
254.760556	3074.886905	17.338765	-0.049230	3.052504
254.518235	3066.891734	17.343770	-0.049179	3.048799
254.620032	3058.902856	17.348775	-0.049193	3.045108
254.451430	3050.945978	17.353779	-0.049156	3.041415
254.482431	3042.959489	17.358784	-0.049157	3.037713
254.658997	3034.963692	17.363789	-0.049185	3.034009
254.371352	3026.946290	17.368794	-0.049126	3.030268
254.346310	3018.976133	17.373799	-0.049116	3.026557
254.607580	3010.971370	17.378803	-0.049159	3.022839
254.425116	3003.000319	17.383808	-0.049120	3.019111
254.450800	2995.050955	17.388813	-0.049120	3.015399
254.262652	2987.042264	17.393818	-0.049079	3.011644
254.381890	2979.055543	17.398823	-0.049096	3.007909
254.255740	2971.080391	17.403827	-0.049068	3.004164
253.893812	2963.133313	17.408832	-0.048995	3.000415
253.952629	2955.171437	17.413837	-0.049001	2.996675
253.908159	2947.130900	17.418842	-0.048987	2.992888
253.771150	2939.152025	17.423847	-0.048957	2.989121
253.860613	2931.146810	17.428851	-0.048968	2.985348
253.813795	2923.193159	17.433856	-0.048954	2.981588
253.654456	2915.231809	17.438861	-0.048919	2.977814
253.565967	2907.207906	17.443866	-0.048898	2.974009
253.590422	2899.213229	17.448871	-0.048897	2.970218
253.551629	2891.257166	17.453875	-0.048884	2.966438
253.402044	2883.278470	17.458880	-0.048851	2.962637
253.408600	2875.330098	17.463885	-0.048847	2.958853
253.235446	2867.333913	17.468890	-0.048810	2.955032
253.297412	2859.325544	17.473895	-0.048816	2.951213
253.231756	2851.327524	17.478899	-0.048799	2.947387
253.413875	2843.324321	17.483904	-0.048827	2.943566
253.340434	2835.364849	17.488909	-0.048809	2.939748
252.985300	2827.437752	17.493914	-0.048737	2.935926
253.217455	2819.390684	17.498919	-0.048775	2.932072
253.097474	2811.419513	17.503923	-0.048748	2.928231
252.946651	2803.442787	17.508928	-0.048714	2.924381
252.894521	2795.509887	17.513933	-0.048699	2.920552
252.853762	2787.509308	17.518938	-0.048687	2.916685
252.756949	2779.475811	17.523943	-0.048663	2.912795
252.589832	2771.461439	17.528947	-0.048627	2.908905
252.615508	2763.461830	17.533952	-0.048627	2.905027
252.664558	2755.543570	17.538957	-0.048631	2.901185
252.462830	2747.567118	17.543962	-0.048588	2.897296
252.509864	2739.595851	17.548967	-0.048591	2.893417
252.481534	2731.592374	17.553971	-0.048581	2.889514
252.242134	2723.623077	17.558976	-0.048531	2.885611
252.378245	2715.673498	17.563981	-0.048551	2.881732
252.309884	2707.669932	17.568986	-0.048533	2.877810
252.230879	2699.698227	17.573991	-0.048513	2.873898
252.094792	2691.695472	17.578995	-0.048483	2.869963
252.141047	2683.699922	17.584000	-0.048486	2.866035
252.032816	2675.754763	17.589005	-0.048461	2.862119
251.646380	2667.781432	17.594010	-0.048384	2.858168
251.791770	2659.822887	17.599015	-0.048405	2.854248
251.767222	2651.816650	17.604019	-0.048396	2.850289
251.793108	2643.824697	17.609024	-0.048395	2.846335
251.961603	2635.866782	17.614029	-0.048421	2.842400
251.715787	2627.889275	17.619034	-0.048370	2.838427
251.583630	2619.924021	17.624039	-0.048341	2.834461
251.628393	2611.905429	17.629043	-0.048344	2.830473
251.584538	2603.921321	17.634048	-0.048330	2.826491
251.407290	2595.971785	17.639053	-0.048292	2.822513
251.414570	2587.981320	17.644058	-0.048288	2.818520
251.616021	2579.993728	17.649063	-0.048321	2.814533
251.378556	2572.025816	17.654067	-0.048271	2.810526
251.172833	2564.045875	17.659072	-0.048228	2.806509
251.290032	2556.080152	17.664077	-0.048244	2.802511
251.204237	2548.110010	17.669082	-0.048223	2.798494
251.050040	2540.154280	17.674087	-0.048189	2.794475
250.875269	2532.140771	17.679091	-0.048151	2.790419
250.955694	2524.135454	17.684096	-0.048161	2.786376
250.839111	2516.203934	17.689101	-0.048134	2.782353
250.764051	2508.228070	17.694106	-0.048115	2.778305
250.674921	2500.267349	17.699111	-0.048093	2.774257
250.779695	2492.244219	17.704115	-0.048107	2.770183
250.717137	2484.281722	17.709120	-0.048091	2.766124
250.858243	2476.312082	17.714125	-0.048112	2.762068
250.795442	2468.329035	17.719130	-0.048095	2.757986
250.653253	2460.348224	17.724135	-0.048063	2.753895
250.461928	2452.311431	17.729139	-0.048022	2.749767
250.455790	2444.344720	17.734144	-0.048016	2.745679
250.557154	2436.397265	17.739149	-0.048029	2.741601
250.325842	2428.437726	17.744154	-0.047981	2.737491
250.334178	2420.467435	17.749159	-0.047978	2.733384
250.328384	2412.469690	17.754163	-0.047971	2.729255
250.185265	2404.507550	17.759168	-0.047939	2.725130
250.277286	2396.557375	17.764173	-0.047951	2.721020
250.123434	2388.600235	17.769178	-0.047917	2.716884
250.176656	2380.597617	17.774183	-0.047922	2.712732
249.996751	2372.621209	17.779187	-0.047883	2.708572
249.918512	2364.633042	17.784192	-0.047864	2.704406
249.991117	2356.691212	17.789197	-0.047872	2.700267
249.746471	2348.731449	17.794202	-0.047821	2.696093
249.732447	2340.727277	17.799207	-0.047813	2.691903
249.851871	2332.739774	17.804211	-0.047830	2.687724
249.495544	2324.801675	17.809216	-0.047759	2.683534
249.460494	2316.861774	17.814221	-0.047747	2.679357
249.368995	2308.867039	17.819226	-0.047725	2.675141
249.197173	2300.879294	17.824231	-0.047688	2.670917
249.266050	2292.865090	17.829235	-0.047695	2.666688
249.128705	2284.899777	17.834240	-0.047664	2.662464
249.288679	2276.936363	17.839245	-0.047689	2.658254
249.110802	2268.979572	17.844250	-0.047651	2.654019
249.057140	2260.982888	17.849255	-0.047635	2.649764
248.921034	2253.045463	17.854259	-0.047605	2.645529
248.779341	2245.079985	17.859264	-0.047573	2.641271
248.724782	2237.137486	17.864269	-0.047558	2.637024
248.849085	2229.103377	17.869274	-0.047576	2.632733
248.781232	2221.134129	17.874279	-0.047558	2.628458
248.725040	2213.171801	17.879283	-0.047542	2.624179
248.576798	2205.205987	17.884288	-0.047510	2.619886
248.589433	2197.265019	17.889293	-0.047507	2.615610
248.566155	2189.247505	17.894298	-0.047497	2.611283
248.639737	2181.273723	17.899303	-0.047506	2.606979
248.510713	2173.341363	17.904307	-0.047476	2.602677
248.348909	2165.388003	17.909312	-0.047441	2.598354
248.219987	2157.404248	17.914317	-0.047412	2.594009
248.188265	2149.239197	17.919322	-0.047401	2.589565
248.228335	2141.304180	17.924327	-0.047403	2.585244
248.086847	2133.392240	17.929331	-0.047371	2.580916
247.879977	2125.463045	17.934336	-0.047328	2.576566
247.898638	2117.506831	17.939341	-0.047326	2.572210
247.730420	2109.537517	17.944346	-0.047289	2.567826
247.791243	2101.563597	17.949351	-0.047296	2.563448
248.037695	2093.585822	17.954355	-0.047336	2.559073
247.658098	2085.656974	17.959360	-0.047260	2.554674
247.729831	2077.679888	17.964365	-0.047269	2.550273
247.668712	2069.695572	17.969370	-0.047252	2.545850
247.685118	2061.739814	17.974375	-0.047250	2.541442
247.527466	2053.798035	17.979379	-0.047215	2.537020
247.340036	2045.838649	17.984384	-0.047175	2.532580
247.184053	2037.884010	17.989389	-0.047141	2.528136
247.143464	2029.909731	17.994394	-0.047128	2.523682
247.347994	2021.926050	17.999399	-0.047161	2.519232
247.311544	2013.974365	18.004403	-0.047149	2.514775
247.005467	2005.990745	18.009408	-0.047087	2.510272
247.139100	1998.008209	18.014413	-0.047106	2.505794
246.869274	1990.071765	18.019418	-0.047051	2.501305
247.004231	1982.107584	18.024423	-0.047071	2.496821
246.833920	1974.137371	18.029427	-0.047034	2.492303
246.770710	1966.144197	18.034432	-0.047017	2.487772
246.979764	1958.177428	18.039437	-0.047051	2.483268
246.833570	1950.225696	18.044442	-0.047018	2.478738
246.659033	1942.302670	18.049447	-0.046981	2.474214
246.774669	1934.297224	18.054451	-0.046997	2.469656
246.736472	1926.313113	18.059456	-0.046985	2.465090
246.546064	1918.411034	18.064461	-0.046944	2.460552
246.289364	1910.459701	18.069466	-0.046891	2.455972
246.363582	1902.476052	18.074471	-0.046900	2.451389
246.337585	1894.509554	18.079475	-0.046890	2.446801
246.196868	1886.542222	18.084480	-0.046858	2.442194
246.159630	1878.620949	18.089485	-0.046846	2.437613
246.016125	1870.626738	18.094490	-0.046814	2.432974
246.125511	1862.595758	18.099495	-0.046829	2.428323
246.022887	1854.665448	18.104499	-0.046805	2.423706
245.831352	1846.718662	18.109504	-0.046764	2.419063
246.056255	1838.759991	18.114509	-0.046801	2.414437
245.870607	1830.792879	18.119514	-0.046761	2.409765
245.773420	1822.851433	18.124519	-0.046738	2.405106
245.596312	1814.921957	18.129523	-0.046699	2.400438
245.396244	1806.980299	18.134528	-0.046657	2.395753
245.676551	1798.963329	18.139533	-0.046704	2.391051
245.511751	1791.012843	18.144538	-0.046668	2.386345
245.350947	1783.073387	18.149543	-0.046633	2.381636
245.222813	1775.148780	18.154547	-0.046604	2.376929
245.265797	1767.144285	18.159552	-0.046607	2.372179
245.133031	1759.203209	18.164557	-0.046577	2.367443
244.826425	1751.273728	18.169562	-0.046514	2.362691
244.955521	1743.307262	18.174567	-0.046533	2.357941
244.917779	1735.343020	18.179571	-0.046521	2.353170
244.805666	1727.354546	18.184576	-0.046495	2.348369
244.858568	1719.398314	18.189581	-0.046500	2.343591
244.854625	1711.440581	18.194586	-0.046494	2.338798
244.640996	1703.518783	18.199591	-0.046449	2.333999
244.521177	1695.561232	18.204595	-0.046421	2.329176
244.601713	1687.584258	18.209600	-0.046431	2.324348
244.515732	1679.652101	18.214605	-0.046410	2.319523
244.231307	1671.739964	18.219610	-0.046352	2.314684
244.423020	1663.705429	18.224615	-0.046382	2.309800
244.316478	1655.772135	18.229619	-0.046357	2.304943
244.179770	1647.826909	18.234624	-0.046326	2.300065
244.209880	1639.893033	18.239629	-0.046327	2.295198
244.132140	1631.919261	18.244634	-0.046307	2.290287
243.927013	1623.993549	18.249639	-0.046264	2.285384
244.094379	1616.036231	18.254643	-0.046290	2.280483
243.984608	1608.104869	18.259648	-0.046264	2.275564
244.184617	1600.050197	18.264653	-0.046296	2.270583
243.773232	1592.124128	18.269658	-0.046214	2.265620
243.811320	1584.186271	18.274663	-0.046216	2.260677
243.922350	1576.239397	18.279667	-0.046232	2.255724
243.716258	1568.289873	18.284672	-0.046188	2.250730
243.662120	1560.354402	18.289677	-0.046173	2.245748
243.520044	1552.423506	18.294682	-0.046141	2.240750
243.581017	1544.474172	18.299687	-0.046147	2.235746
243.399851	1536.536370	18.304691	-0.046108	2.230718
243.412420	1528.554274	18.309696	-0.046106	2.225667
243.210665	1520.645587	18.314701	-0.046063	2.220632
242.929081	1512.730101	18.319706	-0.046005	2.215574
243.206679	1504.723570	18.324711	-0.046052	2.210497
243.172161	1496.781282	18.329715	-0.046040	2.205421
243.053062	1488.865052	18.334720	-0.046013	2.200342
243.115727	1480.926488	18.339725	-0.046019	2.195253
243.087514	1472.919218	18.344730	-0.046009	2.190101
242.864481	1465.012016	18.349735	-0.045962	2.184983
242.700702	1457.091695	18.354739	-0.045926	2.179849
242.660751	1449.144905	18.359744	-0.045914	2.174698
242.627294	1441.198745	18.364749	-0.045902	2.169536
242.583234	1433.243066	18.369754	-0.045889	2.164354
242.760573	1425.295987	18.374759	-0.045917	2.159186
242.749957	1417.373585	18.379763	-0.045910	2.154004
242.407101	1409.433918	18.384768	-0.045841	2.148767
242.435937	1401.497278	18.389773	-0.045841	2.143554
242.292307	1393.576176	18.394778	-0.045809	2.138323
242.217396	1385.640148	18.399783	-0.045790	2.133075
242.109564	1377.700854	18.404787	-0.045764	2.127809
242.080907	1369.745705	18.409792	-0.045754	2.122527
242.193471	1361.824733	18.414797	-0.045770	2.117268
241.945411	1353.852319	18.419802	-0.045718	2.111927
241.909331	1345.892053	18.424807	-0.045706	2.106601
241.818090	1337.973380	18.429811	-0.045684	2.101283
241.812225	1330.033223	18.434816	-0.045678	2.095947
241.644930	1322.114434	18.439821	-0.045642	2.090595
241.456451	1314.177787	18.444826	-0.045601	2.085215
241.534562	1306.257110	18.449831	-0.045611	2.079859
241.665077	1298.319520	18.454835	-0.045630	2.074482
241.706447	1290.349869	18.459840	-0.045632	2.069061
241.601687	1282.446106	18.464845	-0.045608	2.063656
241.320427	1274.550597	18.469850	-0.045550	2.058224
241.237763	1266.621427	18.474855	-0.045529	2.052775
241.191132	1258.689044	18.479859	-0.045516	2.047313
241.013866	1250.774839	18.484864	-0.045477	2.041836
240.919276	1242.869628	18.489869	-0.045455	2.036358
240.919524	1234.889765	18.494874	-0.045449	2.030824
241.003725	1226.935867	18.499879	-0.045460	2.025301
240.661627	1219.071734	18.504883	-0.045391	2.019781
240.603538	1211.142197	18.509888	-0.045375	2.014230
240.418716	1203.223690	18.514893	-0.045335	2.008659
240.680808	1195.238571	18.519898	-0.045379	2.003071
240.440931	1187.368176	18.524903	-0.045329	1.997497
240.694624	1179.387655	18.529907	-0.045371	1.991880
240.643510	1171.448945	18.534912	-0.045357	1.986245
240.395134	1163.581828	18.539917	-0.045305	1.980625
240.241270	1155.680526	18.544922	-0.045271	1.974973
240.445021	1147.701995	18.549927	-0.045304	1.969289
240.375734	1139.805742	18.554931	-0.045286	1.963618
240.127736	1131.927830	18.559936	-0.045235	1.957924
240.214007	1123.981295	18.564941	-0.045246	1.952201
239.951055	1116.049751	18.569946	-0.045191	1.946433
239.822071	1108.143284	18.574951	-0.045162	1.940681
239.830226	1100.224533	18.579955	-0.045159	1.934918
239.566971	1092.312083	18.584960	-0.045104	1.929112
239.626891	1084.394131	18.589965	-0.045110	1.923321
239.596115	1076.475636	18.594970	-0.045099	1.917501
239.493933	1068.576509	18.599975	-0.045075	1.911671
239.364292	1060.663081	18.604979	-0.045046	1.905808
239.333698	1052.737431	18.609984	-0.045035	1.899930
239.425553	1044.827177	18.614989	-0.045047	1.894059
239.193955	1036.926896	18.619994	-0.044999	1.888140
239.113230	1029.027587	18.624999	-0.044979	1.882220
239.086191	1021.134199	18.630003	-0.044968	1.876292
238.814270	1013.234945	18.635008	-0.044913	1.870313
238.856227	1005.306885	18.640013	-0.044915	1.864329
238.746513	997.411531	18.645018	-0.044890	1.858333
238.539011	989.513007	18.650023	-0.044846	1.852304
238.563966	981.592498	18.655027	-0.044845	1.846265
238.366403	973.713825	18.660032	-0.044803	1.840213
238.421678	965.820576	18.665037	-0.044808	1.834159
238.345867	957.894343	18.670042	-0.044789	1.828044
238.145507	950.006361	18.675047	-0.044747	1.821924
238.242673	942.098387	18.680051	-0.044760	1.815802
238.111453	934.194702	18.685056	-0.044730	1.809636
238.245564	926.292622	18.690061	-0.044750	1.803482
238.200308	918.409083	18.695066	-0.044736	1.797300
238.056534	910.491810	18.700071	-0.044704	1.791058
237.970613	902.587529	18.705075	-0.044683	1.784811
237.761967	894.731577	18.710080	-0.044639	1.778566
237.844198	886.831294	18.715085	-0.044649	1.772299
237.823358	878.918195	18.720090	-0.044640	1.765987
237.497252	871.088509	18.725095	-0.044574	1.759681
237.444053	863.213925	18.730099	-0.044559	1.753350
237.285698	855.315769	18.735104	-0.044525	1.746964
237.298087	847.430104	18.740109	-0.044522	1.740587
237.160604	839.564118	18.745114	-0.044491	1.734183
237.153664	831.661687	18.750119	-0.044485	1.727742
237.178668	823.786903	18.755123	-0.044484	1.721303
237.142949	815.910817	18.760128	-0.044472	1.714832
236.997446	808.031052	18.765133	-0.044440	1.708319
236.768303	800.170308	18.770138	-0.044392	1.701785
236.687569	792.311077	18.775143	-0.044372	1.695247
236.844741	784.392114	18.780147	-0.044396	1.688665
236.727272	776.534013	18.785152	-0.044369	1.682072
236.706624	768.678292	18.790157	-0.044360	1.675469
236.419709	760.826451	18.795162	-0.044302	1.668806
236.545980	752.926293	18.800167	-0.044320	1.662131
236.502796	745.079652	18.805171	-0.044307	1.655452
236.080195	737.251845	18.810176	-0.044223	1.648711
236.376416	729.351229	18.815181	-0.044273	1.641977
236.088757	721.532131	18.820186	-0.044214	1.635206
236.007035	713.618364	18.825191	-0.044194	1.628353
235.852775	705.770155	18.830195	-0.044160	1.621518
235.876939	697.903356	18.835200	-0.044159	1.614663
235.872103	690.043562	18.840205	-0.044153	1.607781
235.825975	682.199888	18.845210	-0.044140	1.600877
235.751612	674.368987	18.850215	-0.044121	1.593951
235.612209	666.520248	18.855219	-0.044090	1.586969
235.263077	658.719779	18.860224	-0.044020	1.579969
235.416193	650.851837	18.865229	-0.044043	1.572950
235.315157	643.006927	18.870234	-0.044019	1.565884
235.048629	635.221264	18.875239	-0.043964	1.558815
235.342044	627.313787	18.880243	-0.044014	1.551685
235.180162	619.472725	18.885248	-0.043978	1.544515
234.988062	611.687527	18.890253	-0.043938	1.537359
234.887496	603.850545	18.895258	-0.043914	1.530136
234.839353	596.021017	18.900263	-0.043900	1.522892
234.664710	588.225472	18.905267	-0.043862	1.515627
234.497904	580.391709	18.910272	-0.043826	1.508292
234.484097	572.564897	18.915277	-0.043818	1.500951
234.441267	564.751950	18.920282	-0.043805	1.493583
234.390050	556.917548	18.925287	-0.043790	1.486156
234.262246	549.138075	18.930291	-0.043762	1.478733
234.045994	541.307052	18.935296	-0.043716	1.471208
234.008915	533.482654	18.940301	-0.043704	1.463680
233.880331	525.686572	18.945306	-0.043675	1.456125
233.950200	517.860231	18.950311	-0.043683	1.448534
233.973814	510.053161	18.955315	-0.043682	1.440914
233.734071	502.301783	18.960320	-0.043633	1.433265
233.678221	494.496336	18.965325	-0.043617	1.425552
233.633614	486.711936	18.970330	-0.043604	1.417819
233.342314	478.952696	18.975335	-0.043544	1.410029
233.248026	471.178227	18.980339	-0.043522	1.402212
233.036890	463.420037	18.985344	-0.043477	1.394349
233.086707	455.604176	18.990349	-0.043481	1.386426
232.968504	447.843622	18.995354	-0.043454	1.378486
232.828213	440.076592	19.000359	-0.043423	1.370489
232.839708	432.303751	19.005363	-0.043420	1.362466
232.668868	424.559431	19.010368	-0.043383	1.354393
232.616882	416.795224	19.015373	-0.043369	1.346271
232.554561	409.041919	19.020378	-0.043352	1.338110
232.408802	401.302503	19.025383	-0.043320	1.329899
232.181958	393.593300	19.030387	-0.043272	1.321654
232.149017	385.806655	19.035392	-0.043261	1.313309
232.233157	377.960160	19.040397	-0.043272	1.304867
231.863587	370.287634	19.045402	-0.043198	1.296477
231.933326	362.535974	19.050407	-0.043206	1.288026
232.005860	354.816678	19.055411	-0.043214	1.279556
231.766154	347.129552	19.060416	-0.043165	1.271006
231.717645	339.419539	19.065421	-0.043151	1.262409
231.436726	331.756050	19.070426	-0.043093	1.253761
231.527159	324.027363	19.075431	-0.043105	1.245050
231.363767	316.363400	19.080435	-0.043070	1.236303
231.229426	308.662851	19.085440	-0.043040	1.227457
231.328515	300.961295	19.090445	-0.043053	1.218591
231.031258	293.317104	19.095450	-0.042993	1.209648
230.604864	285.704579	19.100455	-0.042908	1.200651
230.766005	278.002775	19.105459	-0.042933	1.191598
230.457210	270.369306	19.110464	-0.042871	1.182461
230.396578	262.728506	19.115469	-0.042854	1.173296
230.198660	255.093198	19.120474	-0.042813	1.164036
230.204822	247.448455	19.125479	-0.042809	1.154733
229.985645	239.805425	19.130483	-0.042763	1.145310
229.776133	232.196751	19.135488	-0.042719	1.135852
229.682644	224.579811	19.140493	-0.042697	1.126330
229.523672	216.992771	19.145498	-0.042662	1.116750
229.066011	209.447297	19.150503	-0.042572	1.107075
228.996229	201.856913	19.155507	-0.042554	1.097342
228.742927	194.285610	19.160512	-0.042502	1.087505
228.431974	186.756023	19.165517	-0.042439	1.077621
228.321269	179.173824	19.170522	-0.042413	1.067621
228.201592	171.620865	19.175527	-0.042386	1.057563
227.923628	164.097165	19.180531	-0.042330	1.047411
227.620990	156.598393	19.185536	-0.042268	1.037188
227.417144	149.092606	19.190541	-0.042225	1.026876
227.156585	141.607438	19.195546	-0.042172	1.016475
226.849201	134.132223	19.200551	-0.042110	1.005969
226.494783	126.692880	19.205555	-0.042039	0.995391
226.076940	119.219563	19.210560	-0.041956	0.984635
225.844459	111.773679	19.215565	-0.041908	0.973846
225.228255	104.397703	19.220570	-0.041789	0.962940
224.856880	96.997603	19.225575	-0.041715	0.951937
224.288249	89.645287	19.230579	-0.041604	0.940825
223.480885	82.333985	19.235584	-0.041449	0.929578
223.186791	74.961528	19.240589	-0.041389	0.918238
222.698377	67.617104	19.245594	-0.041293	0.906746
222.061685	60.563203	19.250599	-0.041170	0.895523