Tue Mar 23 10:45:32 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.407210	0.019490	0.000000	0.000024	0.721142

0.429447	0.014104	0.005005	0.000020	0.721139
0.590592	-0.013435	0.010010	-0.000010	0.721141
0.458565	0.007851	0.015014	0.000015	0.721137
0.448850	0.011684	0.020019	0.000016	0.721141
0.453587	0.015323	0.025024	0.000016	0.721150
0.550896	-0.009021	0.030029	-0.000003	0.721136
0.604371	-0.016280	0.035034	-0.000013	0.721140
0.520593	-0.126568	0.040038	0.000003	0.720894
0.677055	-0.158389	0.045043	-0.000026	0.720886
0.601378	-0.144003	0.050048	-0.000012	0.720888
0.521953	-0.133826	0.055053	0.000003	0.720880
0.443632	-0.112585	0.060058	0.000017	0.720894
0.425492	-0.112606	0.065062	0.000021	0.720888
0.449309	-0.113871	0.070067	0.000016	0.720894
0.490187	-0.122497	0.075072	0.000009	0.720891
0.331455	-0.094988	0.080077	0.000038	0.720890
0.613008	-0.175686	0.085082	-0.000014	0.720830
0.589782	-0.316439	0.090086	-0.000010	0.720544
0.571007	-0.310915	0.095091	-0.000006	0.720549
0.532253	-0.301161	0.100096	0.000001	0.720554
0.359041	-0.272104	0.105101	0.000033	0.720551
0.649498	-0.322034	0.110106	-0.000021	0.720554
0.529300	-0.347715	0.115110	0.000002	0.720461
0.512111	-0.458846	0.120115	0.000005	0.720237
0.423637	-0.439843	0.125120	0.000021	0.720243
0.358686	-0.434022	0.130125	0.000034	0.720232
0.510246	-0.455144	0.135130	0.000005	0.720243
0.311750	-0.486984	0.140134	0.000042	0.720111
0.332281	-0.591747	0.145139	0.000039	0.719912
0.534462	-0.624657	0.150144	0.000001	0.719918
0.507596	-0.624228	0.155149	0.000006	0.719909
0.317915	-0.627951	0.160154	0.000041	0.719835
0.028020	-0.687258	0.165158	0.000095	0.719616
0.161013	-0.711255	0.170163	0.000071	0.719616
0.183089	-0.712691	0.175168	0.000066	0.719621
-0.013550	-0.743021	0.180173	0.000103	0.719492
0.146581	-0.869824	0.185178	0.000073	0.719298
0.151763	-0.877037	0.190182	0.000072	0.719286
0.159104	-0.876365	0.195187	0.000071	0.719289
0.270636	-1.030123	0.200192	0.000050	0.719025
0.345943	-1.071769	0.205197	0.000036	0.718970
0.252575	-1.047708	0.210202	0.000054	0.718984
0.060721	-1.140864	0.215206	0.000089	0.718733
0.027141	-1.170185	0.220211	0.000096	0.718663
0.131803	-1.189295	0.225216	0.000076	0.718662
-0.052117	-1.277286	0.230221	0.000111	0.718424
-0.040388	-1.304544	0.235226	0.000108	0.718374
-0.106618	-1.295555	0.240230	0.000121	0.718369
-0.001506	-1.467551	0.245235	0.000101	0.718066
0.057681	-1.496613	0.250240	0.000090	0.718029
0.291527	-1.586633	0.255245	0.000047	0.717934
0.043934	-1.648238	0.260250	0.000093	0.717725
-0.224695	-1.602650	0.265254	0.000143	0.717720
-0.097387	-1.750205	0.270259	0.000119	0.717473
-0.169222	-1.771349	0.275264	0.000133	0.717406
-0.209922	-1.815670	0.280269	0.000140	0.717304
-0.260629	-1.909521	0.285274	0.000150	0.717101
-0.379458	-1.892263	0.290278	0.000172	0.717093
-0.312283	-2.053604	0.295283	0.000160	0.716797
-0.562995	-2.021135	0.300288	0.000206	0.716773
-0.787006	-2.065914	0.305293	0.000248	0.716605
-0.678780	-2.153528	0.310298	0.000228	0.716470
-1.578520	-2.013383	0.315302	0.000395	0.716430
-2.496259	-1.981679	0.320307	0.000566	0.716169
-2.680147	-1.949795	0.325312	0.000600	0.716167
-2.732808	-1.961803	0.330317	0.000610	0.716125
-2.521211	-2.114598	0.335322	0.000571	0.715897
-3.091643	-2.016939	0.340326	0.000677	0.715889
-3.384567	-1.970633	0.345331	0.000732	0.715878
-3.464040	-2.116178	0.350336	0.000746	0.715561
-4.128898	-1.998587	0.355341	0.000870	0.715559
-4.212301	-1.981016	0.360346	0.000886	0.715565
-4.298583	-2.072126	0.365350	0.000902	0.715353
-5.373481	-1.932052	0.370355	0.001102	0.715252
-5.529624	-1.897671	0.375360	0.001131	0.715265
-5.261309	-1.953957	0.380365	0.001081	0.715248
-5.124882	-2.054127	0.385370	0.001056	0.715097
-6.352492	-1.923240	0.390374	0.001284	0.714923
-5.828672	-2.016539	0.395379	0.001187	0.714923
-5.929702	-1.992921	0.400384	0.001205	0.714934
-6.418356	-1.916774	0.405389	0.001296	0.714912
-6.578885	-2.029889	0.410394	0.001326	0.714631
-7.072837	-1.941906	0.415398	0.001418	0.714631
-7.126261	-1.937970	0.420403	0.001428	0.714620
-6.925209	-1.967099	0.425408	0.001391	0.714633
-7.282772	-1.907339	0.430413	0.001457	0.714625
-7.470946	-2.037586	0.435418	0.001493	0.714300
-7.984507	-1.940294	0.440422	0.001588	0.714312
-8.283171	-1.894008	0.445427	0.001644	0.714298
-7.562676	-2.021323	0.450432	0.001510	0.714300
-7.676175	-2.006212	0.455437	0.001531	0.714290
-8.208496	-2.024503	0.460442	0.001630	0.714065
-9.015166	-1.919018	0.465446	0.001780	0.713989
-8.602929	-1.994294	0.470451	0.001703	0.713985
-8.470599	-2.014174	0.475456	0.001679	0.713993
-8.778424	-1.965819	0.480461	0.001736	0.713980
-8.555863	-2.018459	0.485466	0.001695	0.713954
-9.455777	-1.998018	0.490470	0.001862	0.713676
-9.524510	-1.989581	0.495475	0.001875	0.713668
-9.495458	-1.992204	0.500480	0.001869	0.713673
-9.559217	-1.986615	0.505485	0.001881	0.713662
-9.588665	-1.978425	0.510490	0.001887	0.713668
-9.718439	-1.973948	0.515494	0.001911	0.713631
-10.185054	-2.021169	0.520499	0.001998	0.713372
-10.187829	-2.018673	0.525504	0.001998	0.713375
-10.777318	-1.918763	0.530509	0.002108	0.713365
-10.151973	-2.024313	0.535514	0.001992	0.713377
-10.132377	-2.029372	0.540518	0.001988	0.713374
-10.396316	-2.008244	0.545523	0.002037	0.713322
-10.745648	-2.088923	0.550528	0.002102	0.713038
-11.006996	-2.042836	0.555533	0.002151	0.713037
-11.336424	-1.983210	0.560538	0.002212	0.713039
-11.311187	-1.989626	0.565542	0.002208	0.713035
-11.206347	-2.010105	0.570547	0.002188	0.713031
-11.122734	-2.023862	0.575552	0.002172	0.713034
-12.147042	-2.000501	0.580557	0.002363	0.712717
-12.076113	-2.009491	0.585562	0.002350	0.712724
-12.369497	-1.960596	0.590566	0.002405	0.712717
-12.369469	-1.959699	0.595571	0.002405	0.712719
-12.379809	-1.953232	0.600576	0.002407	0.712728
-12.316283	-1.971014	0.605581	0.002395	0.712716
-11.903325	-2.054886	0.610586	0.002318	0.712695
-12.860837	-2.035821	0.615590	0.002496	0.712393
-13.071245	-1.999198	0.620595	0.002535	0.712392
-13.080705	-1.994339	0.625600	0.002537	0.712398
-13.474488	-1.926733	0.630605	0.002610	0.712393
-13.172709	-1.977908	0.635610	0.002554	0.712398
-12.997179	-2.011449	0.640614	0.002522	0.712393
-13.156560	-2.000486	0.645619	0.002551	0.712359
-13.683966	-2.037253	0.650624	0.002649	0.712098
-13.942497	-1.991155	0.655629	0.002698	0.712098
-14.126578	-1.950881	0.660634	0.002732	0.712113
-14.447324	-1.889862	0.665638	0.002791	0.712121
-14.384902	-1.899063	0.670643	0.002780	0.712125
-13.979532	-1.968695	0.675648	0.002704	0.712130
-14.351398	-1.911060	0.680653	0.002774	0.712113
-14.330881	-2.029617	0.685658	0.002770	0.711884
-15.295238	-1.911393	0.690662	0.002949	0.711777
-15.290319	-1.911838	0.695667	0.002948	0.711778
-15.339726	-1.895482	0.700672	0.002958	0.711793
-15.481024	-1.875982	0.705677	0.002984	0.711781
-15.055562	-1.948023	0.710682	0.002905	0.711789
-15.206652	-1.925644	0.715686	0.002933	0.711780
-15.490958	-1.873310	0.720691	0.002986	0.711783
-15.003735	-2.074841	0.725696	0.002895	0.711554
-16.301831	-1.881168	0.730701	0.003137	0.711479
-16.357205	-1.866647	0.735706	0.003147	0.711489
-15.733432	-1.975704	0.740710	0.003031	0.711493
-16.345137	-1.871494	0.745715	0.003145	0.711483
-16.399515	-1.857698	0.750720	0.003155	0.711491
-15.977732	-1.944186	0.755725	0.003076	0.711469
-15.603559	-2.077109	0.760730	0.003007	0.711337
-16.992265	-1.920145	0.765734	0.003265	0.711156
-16.965580	-1.923256	0.770739	0.003260	0.711159
-16.578296	-1.993897	0.775744	0.003188	0.711156
-16.892516	-1.941745	0.780749	0.003247	0.711148
-16.849291	-1.943463	0.785754	0.003239	0.711160
-16.820163	-1.948418	0.790758	0.003233	0.711161
-16.844375	-2.035313	0.795763	0.003238	0.710979
-17.370365	-1.983775	0.800768	0.003336	0.710894
-17.413560	-1.981276	0.805773	0.003344	0.710884
-17.366681	-1.982670	0.810778	0.003335	0.710898
-17.945081	-1.878328	0.815782	0.003443	0.710901
-18.048704	-1.860529	0.820787	0.003462	0.710899
-17.392748	-1.978727	0.825792	0.003340	0.710897
-18.350788	-1.976294	0.830797	0.003518	0.710560
-18.773331	-1.898195	0.835802	0.003597	0.710566
-18.323810	-1.986685	0.840806	0.003513	0.710549
-18.343434	-1.983110	0.845811	0.003517	0.710549
-18.344440	-1.980508	0.850816	0.003517	0.710554
-18.629224	-1.934689	0.855821	0.003570	0.710544
-18.144901	-2.046763	0.860826	0.003480	0.710493
-19.286799	-1.972070	0.865830	0.003693	0.710236
-19.209424	-1.989058	0.870835	0.003678	0.710229
-19.033179	-2.018156	0.875840	0.003645	0.710234
-19.367401	-1.962470	0.880845	0.003708	0.710226
-19.391673	-1.952834	0.885850	0.003712	0.710237
-19.375291	-1.957666	0.890854	0.003709	0.710233
-19.171171	-2.083090	0.895859	0.003671	0.710055
-20.363965	-1.940429	0.900864	0.003893	0.709915
-20.308719	-1.957687	0.905869	0.003883	0.709900
-20.153477	-1.980859	0.910874	0.003854	0.709909
-20.564370	-1.906786	0.915878	0.003930	0.709911
-20.795265	-1.870094	0.920883	0.003973	0.709902
-20.176435	-1.975321	0.925888	0.003858	0.709912
-20.375689	-1.973029	0.930893	0.003895	0.709846
-21.723778	-1.833610	0.935898	0.004146	0.709644
-21.432420	-1.891220	0.940902	0.004092	0.709633
-21.509736	-1.884855	0.945907	0.004107	0.709618
-21.092508	-1.959236	0.950912	0.004029	0.709618
-21.375833	-1.910000	0.955917	0.004082	0.709615
-21.154184	-1.951950	0.960922	0.004040	0.709610
-21.285204	-1.927551	0.965926	0.004065	0.709613
-21.284540	-2.026899	0.970931	0.004065	0.709414
-21.988366	-1.963608	0.975936	0.004196	0.709290
-21.749882	-2.012809	0.980941	0.004151	0.709276
-21.769585	-2.005281	0.985946	0.004155	0.709284
-22.239410	-1.923396	0.990950	0.004242	0.709281
-21.879009	-1.990304	0.995955	0.004175	0.709275
-22.002749	-1.965993	1.000960	0.004198	0.709280
-23.049208	-1.931950	1.005965	0.004393	0.708975
-22.770146	-1.983156	1.010970	0.004341	0.708972
-22.909950	-1.955671	1.015974	0.004367	0.708977
-23.127638	-1.918673	1.020979	0.004408	0.708973
-22.914285	-1.952909	1.025984	0.004368	0.708981
-23.093010	-1.926479	1.030989	0.004401	0.708970
-23.418356	-1.857006	1.035994	0.004462	0.708993
-23.322945	-1.964067	1.040998	0.004444	0.708813
-24.300620	-1.863837	1.046003	0.004626	0.708664
-24.022150	-1.909602	1.051008	0.004574	0.708672
-24.036106	-1.913152	1.056013	0.004577	0.708660
-24.095672	-1.898564	1.061018	0.004588	0.708668
-23.803085	-1.956271	1.066022	0.004534	0.708657
-23.969711	-1.930162	1.071027	0.004565	0.708650
-23.863748	-1.970235	1.076032	0.004545	0.708607
-24.718684	-1.938076	1.081037	0.004704	0.708366
-24.584473	-1.957241	1.086042	0.004679	0.708376
-25.071673	-1.868981	1.091046	0.004770	0.708379
-25.141855	-1.855500	1.096051	0.004783	0.708381
-24.829758	-1.911893	1.101056	0.004725	0.708379
-25.238260	-1.842875	1.106061	0.004801	0.708371
-24.906198	-1.898114	1.111066	0.004739	0.708379
-25.012259	-2.009794	1.116070	0.004759	0.708118
-26.507788	-1.782637	1.121075	0.005037	0.708039
-25.714527	-1.926956	1.126080	0.004890	0.708033
-25.219947	-2.020462	1.131085	0.004797	0.708022
-25.723768	-1.924140	1.136090	0.004891	0.708035
-25.855505	-1.899729	1.141094	0.004916	0.708037
-25.759362	-1.915654	1.146099	0.004898	0.708039
-25.720239	-2.029952	1.151104	0.004891	0.707824
-26.976647	-1.852349	1.156109	0.005124	0.707731
-26.387633	-1.960544	1.161114	0.005015	0.707725
-26.422493	-1.953630	1.166118	0.005021	0.707726
-26.935018	-1.860154	1.171123	0.005117	0.707730
-26.687724	-1.895664	1.176128	0.005071	0.707748
-26.974722	-1.845141	1.181133	0.005124	0.707746
-26.935729	-1.938211	1.186138	0.005117	0.707574
-27.672561	-1.892649	1.191142	0.005254	0.707401
-27.463159	-1.932182	1.196147	0.005215	0.707397
-27.588602	-1.903916	1.201152	0.005238	0.707409
-27.545755	-1.921077	1.206157	0.005230	0.707390
-27.141258	-1.989546	1.211162	0.005155	0.707397
-27.179605	-1.980689	1.216166	0.005162	0.707401
-27.686317	-1.993414	1.221171	0.005257	0.707194
-28.457135	-1.899032	1.226176	0.005400	0.707108
-28.218492	-1.945292	1.231181	0.005356	0.707100
-28.257593	-1.934514	1.236186	0.005363	0.707108
-28.308960	-1.929750	1.241190	0.005373	0.707099
-28.335716	-1.926264	1.246195	0.005378	0.707097
-27.883834	-2.003336	1.251200	0.005294	0.707104
-28.775081	-2.004129	1.256205	0.005459	0.706783
-29.234828	-1.927204	1.261210	0.005545	0.706773
-29.115186	-1.952138	1.266214	0.005523	0.706766
-29.230528	-1.933756	1.271219	0.005544	0.706761
-29.234982	-1.925775	1.276224	0.005545	0.706776
-29.411513	-1.897265	1.281229	0.005578	0.706770
-29.181400	-1.936993	1.286234	0.005535	0.706772
-29.694494	-1.985139	1.291238	0.005631	0.706492
-30.331408	-1.885721	1.296243	0.005749	0.706464
-30.137430	-1.917729	1.301248	0.005713	0.706469
-30.467066	-1.852999	1.306253	0.005774	0.706481
-30.162732	-1.915392	1.311258	0.005718	0.706464
-30.067488	-1.928250	1.316262	0.005700	0.706473
-30.478983	-1.850601	1.321267	0.005777	0.706481
-30.481674	-1.902887	1.326272	0.005777	0.706375
-31.293338	-1.870528	1.331277	0.005928	0.706149
-30.859014	-1.945335	1.336282	0.005847	0.706155
-31.239459	-1.880556	1.341286	0.005918	0.706149
-31.297261	-1.875765	1.346291	0.005929	0.706137
-30.339632	-2.042247	1.351296	0.005751	0.706146
-31.113611	-1.903604	1.356301	0.005895	0.706147
-31.322460	-1.908139	1.361306	0.005934	0.706063
-31.459030	-1.972925	1.366310	0.005959	0.705884
-31.575166	-1.955717	1.371315	0.005981	0.705877
-31.683917	-1.932493	1.376320	0.006001	0.705885
-31.505938	-1.970576	1.381325	0.005968	0.705872
-31.291123	-2.005215	1.386330	0.005928	0.705879
-31.896652	-1.906368	1.391334	0.006041	0.705861
-32.845410	-1.892296	1.396339	0.006217	0.705549
-32.512243	-1.952647	1.401344	0.006155	0.705547
-32.804500	-1.905907	1.406349	0.006210	0.705536
-32.690560	-1.922259	1.411354	0.006188	0.705544
-32.146619	-2.020370	1.416358	0.006087	0.705542
-32.749895	-1.914008	1.421363	0.006200	0.705540
-32.675879	-1.957289	1.426368	0.006186	0.705479
-33.533139	-1.929475	1.431373	0.006345	0.705227
-33.179511	-1.989713	1.436378	0.006280	0.705233
-34.054501	-1.824996	1.441382	0.006442	0.705251
-34.060997	-1.827636	1.446387	0.006444	0.705243
-33.374767	-1.950064	1.451392	0.006316	0.705243
-33.925584	-1.846499	1.456397	0.006418	0.705254
-33.884831	-1.856707	1.461402	0.006411	0.705248
-34.027270	-1.925917	1.466406	0.006437	0.705057
-35.351891	-1.745647	1.471411	0.006684	0.704945
-35.107106	-1.781838	1.476416	0.006638	0.704960
-35.136260	-1.787566	1.481421	0.006644	0.704938
-35.260550	-1.759407	1.486426	0.006667	0.704950
-34.872543	-1.841272	1.491430	0.006595	0.704924
-34.918643	-1.831078	1.496435	0.006603	0.704928
-34.690620	-1.862190	1.501440	0.006561	0.704947
-35.021273	-1.819525	1.506445	0.006622	0.704915
-35.655876	-1.848943	1.511450	0.006741	0.704627
-35.447443	-1.885591	1.516454	0.006702	0.704628
-35.510027	-1.880631	1.521459	0.006713	0.704616
-35.379757	-1.905050	1.526464	0.006689	0.704613
-35.689318	-1.850685	1.531469	0.006747	0.704612
-35.175202	-1.941123	1.536474	0.006651	0.704614
-35.229731	-1.968575	1.541478	0.006661	0.704539
-36.580410	-1.849993	1.546483	0.006913	0.704293
-36.220829	-1.911029	1.551488	0.006846	0.704299
-36.492436	-1.868769	1.556493	0.006896	0.704287
-36.347494	-1.896190	1.561498	0.006869	0.704284
-35.986000	-1.961013	1.566502	0.006802	0.704283
-36.029768	-1.955842	1.571507	0.006810	0.704277
-36.256242	-2.023827	1.576512	0.006853	0.704059
-37.226781	-1.897561	1.581517	0.007033	0.703965
-36.783654	-1.973376	1.586522	0.006951	0.703971
-36.748467	-1.979338	1.591526	0.006944	0.703972
-37.419801	-1.864080	1.596531	0.007069	0.703963
-36.737949	-1.981985	1.601536	0.006942	0.703970
-36.824790	-2.047853	1.606541	0.006958	0.703806
-38.140332	-1.891273	1.611546	0.007203	0.703649
-37.740937	-1.962390	1.616550	0.007129	0.703649
-37.565163	-1.997396	1.621555	0.007096	0.703641
-37.678527	-1.974364	1.626560	0.007117	0.703647
-38.072295	-1.905486	1.631565	0.007191	0.703644
-38.080244	-1.901941	1.636570	0.007192	0.703649
-38.298293	-2.006962	1.641574	0.007233	0.703358
-38.629797	-1.954012	1.646579	0.007294	0.703346
-38.598187	-1.952187	1.651584	0.007289	0.703361
-38.881739	-1.902993	1.656589	0.007341	0.703358
-38.721625	-1.933234	1.661594	0.007312	0.703355
-38.496253	-1.973099	1.666598	0.007270	0.703355
-38.609481	-2.037705	1.671603	0.007291	0.703184
-39.741681	-1.915658	1.676608	0.007501	0.703023
-39.771786	-1.912453	1.681613	0.007507	0.703019
-39.528099	-1.954194	1.686618	0.007462	0.703022
-39.498562	-1.959729	1.691622	0.007456	0.703021
-39.840928	-1.902173	1.696627	0.007520	0.703014
-39.544965	-1.950450	1.701632	0.007465	0.703023
-39.672016	-2.021548	1.706637	0.007489	0.702834
-40.912137	-1.860136	1.711642	0.007719	0.702713
-40.484110	-1.933351	1.716646	0.007640	0.702720
-40.603792	-1.917459	1.721651	0.007662	0.702709
-40.664345	-1.903072	1.726656	0.007673	0.702716
-40.548345	-1.928075	1.731661	0.007652	0.702707
-40.660888	-1.907548	1.736666	0.007673	0.702708
-40.554602	-1.983638	1.741670	0.007653	0.702593
-41.636162	-1.894932	1.746675	0.007854	0.702382
-41.209679	-1.962973	1.751680	0.007775	0.702398
-41.206396	-1.971353	1.756685	0.007774	0.702383
-41.802236	-1.856137	1.761690	0.007885	0.702401
-41.258328	-1.959932	1.766694	0.007784	0.702387
-41.593674	-1.900225	1.771699	0.007846	0.702387
-41.433674	-1.990611	1.776704	0.007817	0.702262
-42.513968	-1.885757	1.781709	0.008018	0.702084
-42.294688	-1.920875	1.786714	0.007977	0.702092
-41.954542	-1.981978	1.791718	0.007914	0.702091
-42.371405	-1.911826	1.796723	0.007991	0.702083
-42.077468	-1.961488	1.801728	0.007936	0.702088
-42.306450	-1.921167	1.806733	0.007979	0.702087
-42.223226	-2.035250	1.811738	0.007964	0.701887
-43.090228	-1.944771	1.816742	0.008125	0.701757
-42.948248	-1.971895	1.821747	0.008099	0.701753
-42.919609	-1.974571	1.826752	0.008093	0.701758
-43.328463	-1.905766	1.831757	0.008169	0.701750
-42.984535	-1.964228	1.836762	0.008105	0.701756
-42.834516	-1.991011	1.841766	0.008077	0.701755
-43.777932	-1.969847	1.846771	0.008253	0.701458
-43.879496	-1.953473	1.851776	0.008272	0.701454
-43.991005	-1.936483	1.856781	0.008293	0.701448
-43.677271	-1.990142	1.861786	0.008234	0.701453
-44.014273	-1.928980	1.866790	0.008297	0.701455
-44.333086	-1.873604	1.871795	0.008356	0.701452
-43.703125	-1.994395	1.876800	0.008239	0.701435
-44.606850	-1.981736	1.881805	0.008407	0.701134
-44.881803	-1.932983	1.886810	0.008459	0.701134
-44.815252	-1.943076	1.891814	0.008446	0.701137
-44.603840	-1.984234	1.896819	0.008407	0.701130
-44.894688	-1.928218	1.901824	0.008461	0.701139
-44.888074	-1.934135	1.906829	0.008460	0.701129
-44.797773	-1.970689	1.911834	0.008443	0.701088
-45.413870	-1.958902	1.916838	0.008558	0.700889
-45.429614	-1.957673	1.921843	0.008561	0.700886
-45.177245	-1.997777	1.926848	0.008514	0.700896
-45.681870	-1.912196	1.931853	0.008608	0.700887
-45.490864	-1.944709	1.936858	0.008572	0.700890
-45.214793	-1.993622	1.941862	0.008521	0.700891
-46.066119	-1.987369	1.946867	0.008679	0.700596
-46.596144	-1.914806	1.951872	0.008778	0.700551
-46.392852	-1.954477	1.956877	0.008740	0.700544
-46.202792	-1.989633	1.961882	0.008705	0.700542
-46.682532	-1.901556	1.966886	0.008794	0.700547
-46.636709	-1.915653	1.971891	0.008785	0.700535
-46.036764	-2.021812	1.976896	0.008674	0.700536
-46.956998	-2.011656	1.981901	0.008845	0.700224
-47.566580	-1.900158	1.986906	0.008959	0.700230
-47.262990	-1.952171	1.991910	0.008902	0.700234
-47.177480	-1.971110	1.996915	0.008886	0.700227
-47.452552	-1.919551	2.001920	0.008937	0.700232

-47.191571	-1.997206	2.011917	0.008889	0.700169
-47.966543	-1.985799	2.021914	0.009033	0.699911
-48.291502	-1.927317	2.031910	0.009094	0.699912
-48.081445	-1.963460	2.041907	0.009054	0.699915
-48.473277	-1.889512	2.051904	0.009127	0.699923
-48.180317	-1.945596	2.061901	0.009073	0.699916
-48.245898	-1.936827	2.071898	0.009085	0.699910
-48.114629	-1.907287	2.081894	0.009061	0.700017
-47.374513	-1.933604	2.091891	0.008923	0.700231
-47.458855	-1.917563	2.101888	0.008938	0.700233
-47.333123	-1.939941	2.111885	0.008915	0.700234
-47.109209	-1.979708	2.121882	0.008873	0.700234
-47.383843	-1.930431	2.131878	0.008925	0.700234
-47.374529	-1.933593	2.141875	0.008923	0.700231
-47.324208	-1.942602	2.151872	0.008913	0.700231
-46.645293	-1.928954	2.161869	0.008787	0.700505
-46.434797	-1.944324	2.171866	0.008748	0.700549
-46.271634	-1.975495	2.181862	0.008717	0.700545
-46.428982	-1.947670	2.191859	0.008747	0.700545
-46.261748	-1.974633	2.201856	0.008716	0.700551
-45.293788	-1.984268	2.211853	0.008535	0.700881
-45.350023	-1.973816	2.221850	0.008546	0.700882
-45.192227	-2.002218	2.231846	0.008517	0.700881
-45.453156	-1.956273	2.241843	0.008565	0.700880
-45.293062	-1.931253	2.251840	0.008535	0.700989
-44.784782	-1.950483	2.261837	0.008441	0.701133
-44.888742	-1.931792	2.271834	0.008460	0.701134
-44.732981	-1.957786	2.281830	0.008431	0.701137
-44.048282	-1.927305	2.291827	0.008303	0.701446
-43.840743	-1.963494	2.301824	0.008265	0.701448
-43.711889	-1.984034	2.311821	0.008241	0.701453
-43.773622	-1.903787	2.321818	0.008252	0.701593
-43.011197	-1.961347	2.331814	0.008110	0.701752
-43.081253	-1.950014	2.341811	0.008123	0.701749
-43.157629	-1.924157	2.351808	0.008138	0.701774
-42.293115	-1.924309	2.361805	0.007977	0.702086
-42.050459	-1.969614	2.371802	0.007932	0.702081
-42.213176	-1.941453	2.381798	0.007962	0.702080
-41.806874	-1.932991	2.391795	0.007886	0.702243
-41.190379	-1.975042	2.401792	0.007771	0.702381
-41.197376	-1.974140	2.411789	0.007773	0.702380
-41.427333	-1.927849	2.421786	0.007815	0.702391
-40.387631	-1.959277	2.431782	0.007622	0.702702
-40.548911	-1.930214	2.441779	0.007652	0.702702
-40.462983	-1.944873	2.451776	0.007636	0.702704
-39.967228	-1.943616	2.461773	0.007544	0.702885
-39.531612	-1.954088	2.471770	0.007463	0.703021
-39.657398	-1.931315	2.481766	0.007486	0.703021
-39.751160	-1.888410	2.491763	0.007503	0.703074
-38.847842	-1.908171	2.501760	0.007335	0.703360
-38.751145	-1.923162	2.511757	0.007317	0.703364
-38.782432	-1.920485	2.521754	0.007323	0.703358
-38.101757	-1.924615	2.531750	0.007196	0.703595
-38.108343	-1.896919	2.541747	0.007197	0.703648
-37.877952	-1.934346	2.551744	0.007155	0.703656
-37.646644	-1.908705	2.561741	0.007112	0.703791
-36.961407	-1.942815	2.571738	0.006984	0.703968
-36.989207	-1.939601	2.581734	0.006989	0.703965
-37.240910	-1.889503	2.591731	0.007036	0.703975
-36.361655	-1.892916	2.601728	0.006872	0.704285
-36.252967	-1.913528	2.611725	0.006852	0.704282
-36.111297	-1.938198	2.621722	0.006826	0.704283
-35.710064	-1.913863	2.631718	0.006751	0.704477
-35.540307	-1.876778	2.641715	0.006719	0.704612
-35.147358	-1.950346	2.651712	0.006646	0.704605
-35.377722	-1.886058	2.661709	0.006689	0.704652
-34.323329	-1.949775	2.671706	0.006493	0.704902
-34.632174	-1.893211	2.681702	0.006550	0.704905
-34.327457	-1.947058	2.691699	0.006494	0.704906
-34.000293	-1.903919	2.701696	0.006433	0.705111
-33.449428	-1.943779	2.711693	0.006330	0.705228
-33.400066	-1.951372	2.721690	0.006321	0.705231
-33.623361	-1.901170	2.731686	0.006362	0.705252
-32.589234	-1.946325	2.741683	0.006170	0.705532
-32.259001	-2.002619	2.751680	0.006108	0.705537
-32.670559	-1.927789	2.761677	0.006185	0.705540
-32.493714	-1.888402	2.771674	0.006152	0.705683
-31.644500	-1.945415	2.781670	0.005994	0.705872
-31.604135	-1.952995	2.791667	0.005986	0.705872
-31.645700	-1.942556	2.801664	0.005994	0.705878
-31.323603	-1.892651	2.811661	0.005934	0.706094
-31.104479	-1.901820	2.821658	0.005893	0.706154
-31.158682	-1.896044	2.831654	0.005904	0.706146
-30.549860	-1.900658	2.841651	0.005790	0.706355
-30.200531	-1.906816	2.851648	0.005725	0.706467
-30.267819	-1.895794	2.861645	0.005738	0.706466
-30.065075	-1.867807	2.871642	0.005700	0.706594
-29.388882	-1.902715	2.881638	0.005574	0.706766
-29.508324	-1.882827	2.891635	0.005596	0.706764
-29.243955	-1.905396	2.901632	0.005547	0.706813
-28.584633	-1.879326	2.911629	0.005424	0.707101
-28.457287	-1.903771	2.921626	0.005401	0.707098
-28.502568	-1.895855	2.931622	0.005409	0.707097
-27.700153	-1.932830	2.941619	0.005260	0.707310
-27.838056	-1.863949	2.951616	0.005285	0.707399
-27.390925	-1.947991	2.961613	0.005202	0.707390
-27.328547	-1.937108	2.971610	0.005190	0.707435
-26.624471	-1.922849	2.981606	0.005059	0.707715
-26.467831	-1.952826	2.991603	0.005030	0.707711
-26.351138	-1.972646	3.001600	0.005008	0.707713
-26.326741	-1.923507	3.011597	0.005004	0.707820
-25.551440	-1.959581	3.021594	0.004860	0.708025
-25.731984	-1.927874	3.031590	0.004893	0.708024
-25.692608	-1.933135	3.041587	0.004886	0.708028
-25.150775	-1.886406	3.051584	0.004785	0.708315
-24.726974	-1.937480	3.061581	0.004706	0.708364
-24.747193	-1.931847	3.071578	0.004710	0.708368
-24.947301	-1.845263	3.081574	0.004747	0.708470
-23.873003	-1.945748	3.091571	0.004547	0.708652
-23.984915	-1.925063	3.101568	0.004568	0.708654
-23.866387	-1.946377	3.111565	0.004546	0.708653
-23.447433	-1.880229	3.121562	0.004468	0.708935
-23.189424	-1.908213	3.131558	0.004420	0.708971
-22.987681	-1.944706	3.141555	0.004382	0.708970
-22.972971	-1.873796	3.151552	0.004379	0.709117
-22.047518	-1.954105	3.161549	0.004207	0.709287
-22.330909	-1.903138	3.171546	0.004260	0.709288
-22.345201	-1.893874	3.181542	0.004262	0.709301
-21.747660	-1.835387	3.191539	0.004151	0.709631
-21.505316	-1.885520	3.201536	0.004106	0.709617
-21.264009	-1.927539	3.211533	0.004061	0.709619
-21.078509	-1.850106	3.221530	0.004027	0.709840
-20.553366	-1.909443	3.231526	0.003929	0.709909
-20.489269	-1.923246	3.241523	0.003917	0.709904
-20.373997	-1.907165	3.251520	0.003895	0.709977
-19.506214	-1.933295	3.261517	0.003734	0.710234
-19.704867	-1.900791	3.271514	0.003771	0.710228
-19.750076	-1.893086	3.281510	0.003779	0.710228
-19.023005	-1.903794	3.291507	0.003644	0.710465
-18.724784	-1.917266	3.301504	0.003588	0.710544
-18.498970	-1.956755	3.311501	0.003546	0.710546
-18.672347	-1.924689	3.321498	0.003579	0.710548
-17.940852	-1.888033	3.331494	0.003442	0.710882
-17.763449	-1.920734	3.341491	0.003409	0.710880
-17.579377	-1.952471	3.351488	0.003375	0.710882
-17.588110	-1.902657	3.361485	0.003377	0.710978
-16.954414	-1.927677	3.371482	0.003259	0.711154
-17.016340	-1.917739	3.381478	0.003270	0.711151
-16.963884	-1.925830	3.391475	0.003261	0.711154
-16.259485	-1.912157	3.401472	0.003129	0.711432
-16.284399	-1.886762	3.411469	0.003134	0.711473
-16.050900	-1.930671	3.421466	0.003091	0.711469
-15.791182	-1.902043	3.431462	0.003042	0.711618
-15.369906	-1.898731	3.441459	0.002964	0.711774
-15.299117	-1.908676	3.451456	0.002951	0.711780
-15.214506	-1.905134	3.461453	0.002935	0.711817
-14.666132	-1.856467	3.471450	0.002833	0.712109
-14.264051	-1.928254	3.481446	0.002758	0.712108
-14.321322	-1.919303	3.491443	0.002769	0.712106
-13.919576	-1.902258	3.501440	0.002694	0.712283
-13.274212	-1.958948	3.511437	0.002574	0.712399
-13.409383	-1.935101	3.521434	0.002599	0.712398
-13.444712	-1.930453	3.531430	0.002605	0.712395
-12.861005	-1.871470	3.541427	0.002497	0.712720
-12.410701	-1.952354	3.551424	0.002413	0.712718
-12.566697	-1.923072	3.561421	0.002442	0.712721
-12.254357	-1.903792	3.571418	0.002384	0.712870
-11.354800	-1.982390	3.581414	0.002216	0.713033
-11.518008	-1.954100	3.591411	0.002247	0.713031
-11.460562	-1.963586	3.601408	0.002236	0.713033
-11.025611	-1.927588	3.611405	0.002155	0.713259
-10.388887	-1.984494	3.621402	0.002036	0.713371
-10.444391	-1.975115	3.631398	0.002047	0.713370
-10.567871	-1.954806	3.641395	0.002070	0.713367
-9.479255	-2.033148	3.651392	0.001867	0.713597
-9.681292	-1.963011	3.661389	0.001905	0.713665
-9.500585	-1.996692	3.671386	0.001871	0.713662
-9.398110	-2.015887	3.681382	0.001852	0.713660
-8.925380	-1.970001	3.691379	0.001764	0.713918
-8.606522	-1.995819	3.701376	0.001705	0.713980
-8.829638	-1.956153	3.711373	0.001746	0.713980
-8.546487	-1.986891	3.721370	0.001693	0.714019
-7.885069	-1.969471	3.731366	0.001570	0.714288
-7.640655	-2.013910	3.741363	0.001525	0.714286
-7.789849	-1.986664	3.751360	0.001552	0.714287
-7.439806	-1.953110	3.761357	0.001487	0.714478
-6.494345	-2.050651	3.771354	0.001311	0.714619
-6.893827	-1.980950	3.781350	0.001386	0.714616
-6.826655	-1.993503	3.791347	0.001373	0.714615
-6.096277	-2.005996	3.801344	0.001237	0.714848
-5.933310	-1.998371	3.811341	0.001207	0.714921
-5.678775	-2.045005	3.821338	0.001159	0.714918
-5.991446	-1.987265	3.831334	0.001218	0.714922
-5.362737	-1.940555	3.841331	0.001101	0.715237
-5.093930	-1.987683	3.851328	0.001050	0.715239
-5.102022	-1.984389	3.861325	0.001052	0.715242
-4.454538	-1.997842	3.871322	0.000931	0.715444
-4.307617	-1.969279	3.881318	0.000904	0.715553
-4.460252	-1.938861	3.891315	0.000932	0.715559
-4.150526	-1.965020	3.901312	0.000875	0.715617
-3.393345	-1.956007	3.911309	0.000734	0.715902
-3.012635	-2.028305	3.921306	0.000663	0.715893
-3.430790	-1.952094	3.931302	0.000741	0.715897
-2.761088	-2.010807	3.941299	0.000616	0.716017
-2.452117	-2.002540	3.951296	0.000559	0.716142
-2.515598	-1.989931	3.961293	0.000570	0.716145
-2.318234	-2.025198	3.971290	0.000534	0.716145
-1.907340	-1.942202	3.981286	0.000457	0.716454
-1.736249	-1.972632	3.991283	0.000425	0.716454
-1.692150	-1.980800	4.001280	0.000417	0.716453
-1.792383	-1.844676	4.011277	0.000436	0.716688
-1.195858	-1.910808	4.021274	0.000325	0.716767
-1.298781	-1.892279	4.031270	0.000344	0.716767
-1.172038	-1.762762	4.041267	0.000320	0.717068
-0.802748	-1.816442	4.051264	0.000251	0.717092
-1.165311	-1.694169	4.061261	0.000319	0.717207
-0.904355	-1.644764	4.071258	0.000270	0.717396
-0.946671	-1.606684	4.081254	0.000278	0.717457
-0.888831	-1.488702	4.091251	0.000267	0.717710
-0.667380	-1.486275	4.101248	0.000226	0.717793
-0.649104	-1.369452	4.111245	0.000223	0.718030
-0.549628	-1.314553	4.121242	0.000204	0.718174
-0.466484	-1.234617	4.131238	0.000188	0.718361
-0.527446	-1.116053	4.141235	0.000200	0.718574
-0.377850	-1.076317	4.151232	0.000172	0.718705
-0.370295	-0.940999	4.161229	0.000170	0.718975
-0.074078	-0.890142	4.171226	0.000115	0.719179
-0.285565	-0.759233	4.181222	0.000154	0.719363
-0.383096	-0.612211	4.191219	0.000172	0.719619
-0.234631	-0.498161	4.201216	0.000145	0.719896
-0.132382	-0.395499	4.211213	0.000126	0.720134
-0.006820	-0.295241	4.221210	0.000102	0.720375
-0.006198	-0.161862	4.231206	0.000102	0.720638
0.180575	-0.055184	4.241203	0.000067	0.720914
0.139579	0.066244	4.251200	0.000075	0.721138
0.000000	0.284563	4.261197	0.000101	0.721519

0.050086	0.896550	4.266202	0.000091	0.722739
0.433158	2.090037	4.271206	0.000019	0.725212
0.808447	3.880820	4.276211	-0.000052	0.728837
0.927523	6.266944	4.281216	-0.000076	0.733509
1.420723	9.097751	4.286221	-0.000170	0.739133
1.686216	12.451883	4.291226	-0.000221	0.745634
2.144534	16.226467	4.296230	-0.000309	0.752937
2.835099	20.367334	4.301235	-0.000440	0.760929
3.207561	24.962459	4.306240	-0.000513	0.769571
3.646374	29.921881	4.311245	-0.000598	0.778803
4.007521	35.234070	4.316250	-0.000668	0.788537
4.759569	40.798173	4.321254	-0.000812	0.798722
5.698965	46.637579	4.326259	-0.000991	0.809320
6.251391	52.832442	4.331264	-0.001098	0.820277
6.791992	59.305420	4.336269	-0.001203	0.831560
7.392250	65.985784	4.341274	-0.001319	0.843059
7.886423	72.913806	4.346278	-0.001415	0.854782
8.918834	79.956926	4.351283	-0.001612	0.866691
9.313777	87.295550	4.356288	-0.001690	0.878733
10.075040	94.745413	4.361293	-0.001837	0.890892
10.924758	102.341896	4.366298	-0.002000	0.903142
11.547968	110.133509	4.371302	-0.002121	0.915468
11.972673	118.065194	4.376307	-0.002205	0.927791
12.266418	126.134151	4.381312	-0.002265	0.940124
12.926126	134.248154	4.386317	-0.002394	0.952460
13.583383	142.438502	4.391322	-0.002521	0.964750
15.330564	150.539587	4.396326	-0.002852	0.977031
16.113073	158.916671	4.401331	-0.003003	0.989313
16.780748	167.341496	4.406336	-0.003133	1.001483
17.553796	175.810347	4.411341	-0.003282	1.013594
17.759592	184.394950	4.416346	-0.003326	1.025586
18.921500	192.871916	4.421350	-0.003548	1.037518
19.736367	201.432449	4.426355	-0.003705	1.049346
20.075316	210.084662	4.431360	-0.003774	1.061054
20.972814	218.671783	4.436365	-0.003947	1.072675
21.840720	227.261355	4.441370	-0.004114	1.084168
22.182426	235.958427	4.446374	-0.004183	1.095561
23.107818	244.552374	4.451379	-0.004361	1.106834
23.960294	253.167693	4.456384	-0.004526	1.118004
24.360233	261.865614	4.461389	-0.004606	1.129069
24.663736	270.568002	4.466394	-0.004668	1.140011
25.150417	279.251022	4.471398	-0.004764	1.150864
25.794706	287.882134	4.476403	-0.004890	1.161585
26.267195	296.510422	4.481408	-0.004983	1.172168
27.169047	305.066255	4.486413	-0.005157	1.182657
27.861547	313.653379	4.491418	-0.005291	1.193049
28.028972	322.305658	4.496422	-0.005328	1.203322
28.517052	330.900352	4.501427	-0.005425	1.213504
28.958055	339.477090	4.506432	-0.005512	1.223571
28.978975	348.152759	4.511437	-0.005522	1.233588
29.326355	356.685425	4.516442	-0.005592	1.243424
29.996364	365.173510	4.521446	-0.005722	1.253194
30.482059	373.695533	4.526451	-0.005818	1.262891
30.976217	382.192089	4.531456	-0.005916	1.272487
31.492285	390.673267	4.536461	-0.006018	1.281998
32.565942	399.065531	4.541466	-0.006223	1.291444
33.330845	407.501881	4.546470	-0.006371	1.300813
33.825863	416.029889	4.551475	-0.006469	1.310165
34.483579	424.521201	4.556480	-0.006597	1.319439
34.706839	433.000340	4.561485	-0.006644	1.328559
35.131141	441.411255	4.566490	-0.006728	1.337579
35.503815	449.814902	4.571494	-0.006803	1.346522
35.839592	458.253447	4.576499	-0.006871	1.355436
36.080992	466.637720	4.581504	-0.006922	1.364218
36.465747	475.035584	4.586509	-0.006999	1.372983
37.083853	483.353342	4.591514	-0.007119	1.381650
37.379172	491.746379	4.596518	-0.007180	1.390285
37.851724	500.110703	4.601523	-0.007273	1.398867
38.423822	508.404393	4.606528	-0.007385	1.407342
39.200650	516.705326	4.611533	-0.007535	1.415807
40.884841	524.835325	4.616538	-0.007854	1.424200
40.999873	533.258098	4.621542	-0.007881	1.432577
41.489064	541.588675	4.626547	-0.007977	1.440875
41.657875	549.957233	4.631552	-0.008014	1.449111
41.980563	558.314101	4.636557	-0.008080	1.457314
42.673055	566.574134	4.641562	-0.008214	1.465436
46.711256	574.387357	4.646566	-0.008971	1.473610
48.117347	582.628998	4.651571	-0.009238	1.481736
48.515711	591.008550	4.656576	-0.009318	1.489791
48.836500	599.400694	4.661581	-0.009383	1.497802
49.032886	607.757549	4.666586	-0.009425	1.505718
49.206691	616.135386	4.671590	-0.009463	1.513609
49.831564	624.402087	4.676595	-0.009585	1.521424
50.086260	632.706763	4.681600	-0.009638	1.529178
50.561671	641.000225	4.686605	-0.009731	1.536916
51.085062	649.243462	4.691610	-0.009834	1.544575
51.519113	657.528251	4.696614	-0.009921	1.552222
51.894548	665.793341	4.701619	-0.009996	1.559804
52.325908	674.012094	4.706624	-0.010081	1.567316
53.241487	682.199716	4.711629	-0.010257	1.574834
53.711227	690.433864	4.716634	-0.010350	1.582293
54.165413	698.681610	4.721638	-0.010440	1.589727
54.946391	706.868200	4.726643	-0.010591	1.597118
55.190131	715.117293	4.731648	-0.010642	1.604455
55.578881	723.369525	4.736653	-0.010719	1.611781
56.025857	731.594298	4.741658	-0.010808	1.619057
56.282828	739.828054	4.746662	-0.010861	1.626283
56.793592	748.094794	4.751667	-0.010962	1.633540
57.274776	756.261918	4.756672	-0.011057	1.640675
58.482297	764.340627	4.761677	-0.011287	1.647802
59.033554	772.543638	4.766682	-0.011395	1.654915
59.335433	780.757559	4.771686	-0.011456	1.661973
59.954436	788.943414	4.776691	-0.011577	1.669019
60.162745	797.178674	4.781696	-0.011621	1.676023
60.769511	805.321447	4.786701	-0.011739	1.682973
61.227714	813.516085	4.791706	-0.011830	1.689918
61.606729	821.720252	4.796710	-0.011906	1.696831
62.379135	829.852202	4.801715	-0.012055	1.703708
63.163812	838.005748	4.806720	-0.012206	1.710577
63.641459	846.220565	4.811725	-0.012301	1.717428
64.139673	854.384554	4.816730	-0.012399	1.724213
64.814885	862.525458	4.821734	-0.012530	1.730976
65.518050	870.698378	4.826739	-0.012666	1.737741
65.948689	878.838873	4.831744	-0.012752	1.744419
66.346541	887.044908	4.836749	-0.012831	1.751120
66.835356	895.220196	4.841754	-0.012927	1.757782
67.106185	903.392544	4.846758	-0.012983	1.764389
67.651696	911.559528	4.851763	-0.013090	1.771001
67.958234	919.746557	4.856768	-0.013152	1.777575
68.450112	927.898105	4.861773	-0.013249	1.784119
68.916564	936.087197	4.866778	-0.013341	1.790666
69.344484	944.267354	4.871782	-0.013426	1.797177
69.924905	952.379701	4.876787	-0.013540	1.803629
70.541599	960.495739	4.881792	-0.013660	1.810066
70.631946	968.717047	4.886797	-0.013682	1.816498
71.347053	976.780989	4.891802	-0.013820	1.822860
71.852695	984.916507	4.896806	-0.013920	1.829231
72.298961	993.072209	4.901811	-0.014008	1.835587
72.685185	1001.188899	4.906816	-0.014086	1.841885
73.066260	1009.335970	4.911821	-0.014162	1.848183
73.596064	1017.486415	4.916826	-0.014266	1.854480
74.105539	1025.597429	4.921830	-0.014366	1.860723
74.731534	1033.727864	4.926835	-0.014488	1.866973
75.683614	1041.809607	4.931840	-0.014670	1.873203
76.107041	1049.984076	4.936845	-0.014755	1.879422
76.411258	1058.115814	4.941850	-0.014816	1.885574
76.923014	1066.243112	4.946854	-0.014917	1.891726
77.479197	1074.366141	4.951859	-0.015026	1.897859
77.800297	1082.494686	4.956864	-0.015091	1.903951
78.740544	1090.568377	4.961869	-0.015271	1.910052
79.547218	1098.679617	4.966874	-0.015427	1.916145
79.892312	1106.825996	4.971878	-0.015496	1.922194
80.512789	1114.942648	4.976883	-0.015617	1.928233
81.042109	1123.077910	4.981888	-0.015721	1.934256
81.356243	1131.229840	4.986893	-0.015785	1.940248
81.720276	1139.360089	4.991898	-0.015858	1.946212
82.382862	1147.491336	4.996902	-0.015987	1.952191
83.216326	1155.592532	5.001907	-0.016147	1.958148
83.725774	1163.679412	5.006912	-0.016247	1.964041
84.212958	1171.793056	5.011917	-0.016343	1.969934
84.423305	1179.968107	5.016922	-0.016388	1.975823
84.710001	1188.073797	5.021926	-0.016446	1.981653
85.247944	1196.176144	5.026931	-0.016552	1.987490
85.673479	1204.287159	5.031936	-0.016636	1.993304
86.301938	1212.368792	5.036941	-0.016759	1.999102
86.805284	1220.466198	5.041946	-0.016858	2.004881
87.497324	1228.522490	5.046950	-0.016992	2.010634
88.309035	1236.616797	5.051955	-0.017148	2.016409
88.407682	1244.777905	5.056960	-0.017172	2.022141
88.606926	1252.936504	5.061965	-0.017214	2.027865
89.199122	1261.045768	5.066970	-0.017330	2.033578
89.400672	1269.166884	5.071974	-0.017373	2.039244
90.028002	1277.219253	5.076979	-0.017495	2.044890
90.584148	1285.294873	5.081984	-0.017603	2.050529
91.289571	1293.378391	5.086989	-0.017740	2.056173
91.592952	1301.499983	5.091994	-0.017802	2.061787
92.009774	1309.598703	5.096998	-0.017885	2.067381
92.663876	1317.708016	5.102003	-0.018012	2.072991
92.716407	1325.848695	5.107008	-0.018027	2.078548
93.402238	1333.902695	5.112013	-0.018160	2.084093
93.957060	1341.990099	5.117018	-0.018268	2.089633
94.291337	1350.114953	5.122022	-0.018336	2.095162
94.657930	1358.215405	5.127027	-0.018410	2.100663
95.255990	1366.277250	5.132032	-0.018526	2.106146
95.823462	1374.417863	5.137037	-0.018637	2.111664
96.267003	1382.551147	5.142042	-0.018725	2.117151
96.860823	1390.577991	5.147046	-0.018841	2.122567
97.707939	1398.609377	5.152051	-0.019004	2.127997
98.165162	1406.706805	5.157056	-0.019094	2.133419
98.904104	1414.761020	5.162061	-0.019237	2.138825
99.804542	1422.804815	5.167066	-0.019410	2.144226
100.313852	1430.905069	5.172070	-0.019510	2.149614
100.613454	1439.069745	5.177075	-0.019571	2.155010
101.111796	1447.133409	5.182080	-0.019669	2.160346
101.869626	1455.176426	5.187085	-0.019816	2.165678
102.436594	1463.290910	5.192090	-0.019926	2.171027
102.615802	1471.446034	5.197094	-0.019965	2.176352
103.254488	1479.513847	5.202099	-0.020089	2.181651
103.401075	1487.612018	5.207104	-0.020122	2.186910
103.647753	1495.772260	5.212109	-0.020173	2.192207
104.276016	1503.819829	5.217114	-0.020295	2.197452
104.662139	1511.866293	5.222118	-0.020372	2.202663
105.023128	1519.966087	5.227123	-0.020445	2.207892
105.396938	1528.048163	5.232128	-0.020520	2.213100
105.927415	1536.118533	5.237133	-0.020624	2.218301
106.587587	1544.155248	5.242138	-0.020752	2.223480
106.821013	1552.263501	5.247142	-0.020801	2.228655
107.402887	1560.365284	5.252147	-0.020914	2.233844
107.794664	1568.415033	5.257152	-0.020993	2.238971
108.268690	1576.487178	5.262157	-0.021086	2.244108
108.956032	1584.532626	5.267162	-0.021219	2.249235
109.095647	1592.682447	5.272166	-0.021251	2.254368
109.504068	1600.757842	5.277171	-0.021332	2.259466
109.931626	1608.822644	5.282176	-0.021417	2.264548
110.531127	1616.867328	5.287181	-0.021534	2.269620
111.185087	1625.021061	5.292186	-0.021661	2.274753
111.347203	1633.096988	5.297190	-0.021696	2.279784
111.594262	1641.177926	5.302195	-0.021747	2.284814
111.908162	1649.234067	5.307200	-0.021811	2.289824
112.177274	1657.324359	5.312205	-0.021867	2.294840
112.706499	1665.359592	5.317210	-0.021970	2.299833
113.052052	1673.402712	5.322214	-0.022040	2.304804
113.581069	1681.471250	5.327219	-0.022144	2.309795
113.789400	1689.586065	5.332224	-0.022188	2.314777
114.338436	1697.629082	5.337229	-0.022295	2.319733
114.735021	1705.688119	5.342234	-0.022374	2.324676
114.931675	1713.789445	5.347238	-0.022416	2.329616
115.334279	1721.870898	5.352243	-0.022496	2.334552
115.526813	1729.937020	5.357248	-0.022538	2.339450
115.862526	1738.012717	5.362253	-0.022605	2.344355
116.542115	1746.037077	5.367258	-0.022737	2.349248
116.875771	1754.139332	5.372262	-0.022804	2.354148
117.188532	1762.223254	5.377267	-0.022868	2.359026
117.505909	1770.256988	5.382272	-0.022932	2.363864
117.944422	1778.307342	5.387277	-0.023019	2.368711
118.411841	1786.384761	5.392282	-0.023111	2.373567
118.587517	1794.465620	5.397286	-0.023149	2.378392
119.045184	1802.503743	5.402291	-0.023240	2.383204
119.565293	1810.564850	5.407296	-0.023342	2.388025
119.930119	1818.668852	5.412301	-0.023415	2.392849
120.337986	1826.750920	5.417306	-0.023496	2.397653
121.327784	1834.705844	5.422310	-0.023686	2.402419
121.832005	1842.796405	5.427315	-0.023785	2.407217
122.411252	1850.840268	5.432320	-0.023898	2.411983
122.783062	1858.932152	5.437325	-0.023973	2.416752
123.300347	1866.976687	5.442330	-0.024074	2.421495
123.428250	1875.065151	5.447334	-0.024103	2.426225
124.077467	1883.148042	5.452339	-0.024229	2.430981
124.260305	1891.315805	5.457344	-0.024269	2.435742
124.846650	1899.296377	5.462349	-0.024383	2.440416
125.299383	1907.322034	5.467354	-0.024473	2.445097
125.825156	1915.340560	5.472358	-0.024576	2.449770
126.277715	1923.442298	5.477363	-0.024665	2.454477
126.471916	1931.511096	5.482368	-0.024707	2.459136
127.080358	1939.540522	5.487373	-0.024825	2.463795
127.421006	1947.617403	5.492378	-0.024894	2.468452
127.757968	1955.695775	5.497382	-0.024962	2.473100
128.288558	1963.745031	5.502387	-0.025066	2.477738
128.758257	1971.766363	5.507392	-0.025159	2.482346
128.949021	1979.866445	5.512397	-0.025200	2.486970
129.419493	1987.921404	5.517402	-0.025292	2.491581
129.552289	1996.018879	5.522406	-0.025322	2.496182
130.099366	2004.043536	5.527411	-0.025430	2.500763
130.429544	2012.087642	5.532416	-0.025496	2.505331
130.837883	2020.158504	5.537421	-0.025578	2.509912
131.309735	2028.268161	5.542426	-0.025671	2.514511
131.549620	2036.312528	5.547430	-0.025721	2.519047
132.252441	2044.308506	5.552435	-0.025857	2.523582
132.535839	2052.387337	5.557440	-0.025915	2.528125
133.015465	2060.442748	5.562445	-0.026009	2.532660
133.227193	2068.537736	5.567450	-0.026054	2.537190
133.508321	2076.557423	5.572454	-0.026112	2.541675
133.833814	2084.641494	5.577459	-0.026177	2.546191
134.106389	2092.706275	5.582464	-0.026233	2.550685
134.251150	2100.794840	5.587469	-0.026266	2.555174
134.281301	2108.869803	5.592474	-0.026277	2.559641
134.476139	2116.872753	5.597478	-0.026318	2.564071
134.820809	2124.930660	5.602483	-0.026387	2.568534
135.111798	2132.985116	5.607488	-0.026447	2.572984
135.484272	2141.029539	5.612493	-0.026521	2.577426
135.550381	2149.127007	5.617498	-0.026539	2.581869
135.855749	2157.163729	5.622502	-0.026601	2.586286
136.715623	2165.150327	5.627507	-0.026766	2.590707
137.098926	2173.382990	5.632512	-0.026843	2.595222
137.575264	2181.333624	5.637517	-0.026937	2.599582
137.922669	2189.369983	5.642522	-0.027007	2.603972
137.889520	2197.416630	5.647526	-0.027006	2.608335
138.395468	2205.466529	5.652531	-0.027106	2.612728
138.784197	2213.492767	5.657536	-0.027183	2.617093
138.759657	2221.572368	5.662541	-0.027184	2.621452
139.281509	2229.576912	5.667546	-0.027286	2.625800
139.504429	2237.625434	5.672550	-0.027333	2.630144
139.645645	2245.731478	5.677555	-0.027365	2.634507
139.917744	2253.748457	5.682560	-0.027420	2.638823
140.156313	2261.790718	5.687565	-0.027470	2.643143
140.536875	2269.829806	5.692570	-0.027546	2.647464
140.832731	2277.874739	5.697574	-0.027607	2.651775
140.980951	2285.970590	5.702579	-0.027639	2.656097
141.257468	2293.975393	5.707584	-0.027696	2.660372
141.356589	2302.031266	5.712589	-0.027720	2.664655
141.737685	2310.093681	5.717594	-0.027796	2.668953
142.139549	2318.135520	5.722598	-0.027876	2.673235
142.330129	2326.205981	5.727603	-0.027917	2.677511
142.488322	2334.225849	5.732608	-0.027951	2.681752
142.995357	2342.234876	5.737613	-0.028051	2.686002
143.288753	2350.308735	5.742618	-0.028111	2.690266
143.461099	2358.379172	5.747622	-0.028148	2.694514
143.982817	2366.399707	5.752627	-0.028251	2.698751
144.021741	2374.494524	5.757632	-0.028263	2.702989
144.291293	2382.528479	5.762637	-0.028319	2.707204
144.636900	2390.561854	5.767642	-0.028388	2.711417
144.975868	2398.617118	5.772646	-0.028457	2.715633
145.431962	2406.610505	5.777651	-0.028547	2.719819
145.513431	2414.675986	5.782656	-0.028567	2.724012
145.729881	2422.746391	5.787661	-0.028613	2.728209
146.031957	2430.814401	5.792666	-0.028674	2.732404
146.208788	2438.879560	5.797670	-0.028712	2.736584
146.476453	2446.921021	5.802675	-0.028768	2.740750
146.713739	2454.951777	5.807680	-0.028817	2.744903
147.099644	2462.968872	5.812685	-0.028894	2.749051
147.399253	2471.097831	5.817690	-0.028955	2.753245
147.581922	2479.126978	5.822694	-0.028994	2.757375
148.122239	2487.106934	5.827699	-0.029100	2.761494
148.331653	2495.121862	5.832704	-0.029144	2.765605
148.615318	2503.154263	5.837709	-0.029202	2.769724
149.427185	2511.181461	5.842714	-0.029359	2.773865
149.578982	2519.221072	5.847718	-0.029392	2.777967
149.750187	2527.299295	5.852723	-0.029429	2.782084
149.633390	2535.378607	5.857728	-0.029413	2.786178
150.213862	2543.379315	5.862733	-0.029526	2.790267
150.894437	2551.417589	5.867738	-0.029658	2.794375
151.015379	2559.458955	5.872742	-0.029686	2.798446
151.480592	2567.474388	5.877747	-0.029778	2.802517
151.716410	2575.546673	5.882752	-0.029827	2.806599
151.905599	2583.587756	5.887757	-0.029867	2.810655
152.493677	2591.649676	5.892762	-0.029982	2.814740
152.670989	2599.682106	5.897766	-0.030020	2.818779
152.989961	2607.720624	5.902771	-0.030085	2.822825
153.381368	2615.741383	5.907776	-0.030163	2.826859
153.469046	2623.840219	5.912781	-0.030185	2.830910
153.835647	2631.912199	5.917786	-0.030258	2.834957
153.871923	2639.925425	5.922790	-0.030270	2.838950
154.364838	2647.926635	5.927795	-0.030367	2.842957
154.544879	2655.976589	5.932800	-0.030406	2.846966
154.853674	2664.010902	5.937805	-0.030469	2.850968
155.093716	2672.085226	5.942810	-0.030519	2.854980
155.554559	2680.084372	5.947814	-0.030610	2.858962
155.980761	2688.122848	5.952819	-0.030694	2.862956
156.238428	2696.172629	5.957824	-0.030748	2.866940
156.439612	2704.233718	5.962829	-0.030790	2.870921
156.877609	2712.277827	5.967834	-0.030877	2.874901
157.081457	2720.296396	5.972838	-0.030920	2.878851
157.637579	2728.326483	5.977843	-0.031029	2.882819
157.904643	2736.371274	5.982848	-0.031084	2.886774
157.872718	2744.442439	5.987853	-0.031083	2.890720
158.237581	2752.509592	5.992858	-0.031157	2.894680
158.366137	2760.549995	5.997862	-0.031186	2.898609
158.598264	2768.576519	6.002867	-0.031234	2.902531
158.547592	2776.666930	6.007872	-0.031230	2.906464
158.943866	2784.670402	6.012877	-0.031309	2.910373
159.344063	2792.795838	6.017882	-0.031389	2.914336
159.348092	2800.781733	6.022886	-0.031395	2.918205
159.939463	2808.771013	6.027891	-0.031510	2.922101
160.306923	2816.758801	6.032896	-0.031584	2.925980
160.560380	2824.780137	6.037901	-0.031636	2.929864
160.669050	2832.888256	6.042906	-0.031662	2.933777
160.843742	2840.920919	6.047910	-0.031699	2.937652
161.462784	2848.927324	6.052915	-0.031820	2.941532
161.660334	2856.952350	6.057920	-0.031862	2.945393
162.033862	2864.984066	6.062925	-0.031937	2.949263
162.116193	2873.102208	6.067930	-0.031957	2.953153
162.393348	2881.093236	6.072934	-0.032014	2.956987
162.756960	2889.124793	6.077939	-0.032087	2.960841
162.979115	2897.137580	6.082944	-0.032134	2.964672
163.190267	2905.168594	6.087949	-0.032178	2.968508
163.482699	2913.259921	6.092954	-0.032238	2.972370
163.800177	2921.305998	6.097958	-0.032302	2.976208
164.259372	2929.304134	6.102963	-0.032393	2.980025
164.665554	2937.328941	6.107968	-0.032474	2.983847
164.757935	2945.371673	6.112973	-0.032496	2.987657
165.104467	2953.428989	6.117978	-0.032566	2.991481
165.462394	2961.494284	6.122982	-0.032638	2.995305
165.598602	2969.503901	6.127987	-0.032669	2.999087
166.206123	2977.474927	6.132992	-0.032787	3.002869
166.318634	2985.544708	6.137997	-0.032813	3.006668
166.742017	2993.576306	6.143002	-0.032897	3.010459
166.904536	3001.617489	6.148006	-0.032933	3.014238
167.274606	3009.675262	6.153011	-0.033007	3.018030
167.456612	3017.721504	6.158016	-0.033046	3.021802
167.836397	3025.720609	6.163021	-0.033122	3.025557
168.537955	3033.752121	6.168026	-0.033258	3.029338
168.681763	3041.820833	6.173030	-0.033290	3.033105
169.119002	3049.872083	6.178035	-0.033376	3.036873
169.388770	3057.866794	6.183040	-0.033432	3.040602
169.465727	3065.914826	6.188045	-0.033451	3.044342
169.659214	3073.981740	6.193050	-0.033493	3.048091
169.919733	3082.014059	6.198054	-0.033546	3.051823
170.131311	3090.054597	6.203059	-0.033591	3.055552
170.478524	3098.078398	6.208064	-0.033661	3.059275
170.714940	3106.095674	6.213069	-0.033710	3.062985
171.256866	3114.124992	6.218074	-0.033816	3.066711
171.395753	3122.188923	6.223078	-0.033847	3.070429
171.738897	3130.293691	6.228083	-0.033917	3.074170
172.285817	3138.262075	6.233088	-0.034024	3.077854
172.385989	3146.301658	6.238093	-0.034048	3.081546
172.647528	3154.289700	6.243098	-0.034101	3.085217
172.883540	3162.328879	6.248102	-0.034151	3.088905
173.278499	3170.371446	6.253107	-0.034229	3.092598
173.340932	3178.411221	6.258112	-0.034246	3.096270
173.438798	3186.439912	6.263117	-0.034270	3.099935
173.887485	3194.472726	6.268122	-0.034359	3.103613
174.352377	3202.460115	6.273126	-0.034450	3.107266
174.907387	3210.508731	6.278131	-0.034559	3.110947
175.229306	3218.569589	6.283136	-0.034624	3.114618
175.469521	3226.568234	6.288141	-0.034674	3.118253
175.760339	3234.618976	6.293146	-0.034733	3.121910
176.046421	3242.619661	6.298150	-0.034792	3.125540
176.538627	3250.666286	6.303155	-0.034889	3.129195
176.680890	3258.742328	6.308160	-0.034921	3.132844
176.748593	3266.826143	6.313165	-0.034938	3.136488
176.918680	3274.834431	6.318170	-0.034975	3.140099
177.131454	3282.832581	6.323174	-0.035020	3.143703
177.403798	3290.888507	6.328179	-0.035076	3.147332
177.685081	3298.912602	6.333184	-0.035134	3.150942
177.781058	3306.968176	6.338189	-0.035157	3.154554
177.924843	3315.002585	6.343194	-0.035189	3.158155
178.085727	3323.009640	6.348198	-0.035224	3.161740
178.386963	3331.006765	6.353203	-0.035285	3.165322
178.548042	3339.066506	6.358208	-0.035321	3.168923
178.923857	3347.065818	6.363213	-0.035396	3.172501
179.513112	3355.131893	6.368218	-0.035511	3.176114
179.462879	3363.167959	6.373222	-0.035507	3.179683
179.477174	3371.196331	6.378227	-0.035514	3.183246
180.019752	3379.203931	6.383232	-0.035621	3.186819
180.435082	3387.204650	6.388237	-0.035703	3.190380
180.642046	3395.298511	6.393242	-0.035747	3.193968
180.727428	3403.316211	6.398246	-0.035768	3.197514
180.949067	3411.378854	6.403251	-0.035815	3.201082
181.104743	3419.368948	6.408256	-0.035849	3.204611
181.366401	3427.382813	6.413261	-0.035903	3.208150
181.817622	3435.447562	6.418266	-0.035992	3.211716
181.631622	3443.504291	6.423270	-0.035963	3.215248
181.872683	3451.527109	6.428275	-0.036013	3.218779
182.197298	3459.532560	6.433280	-0.036079	3.222302
182.660465	3467.537635	6.438285	-0.036170	3.225827
182.972126	3475.591452	6.443290	-0.036233	3.229362
183.040644	3483.666740	6.448294	-0.036251	3.232894
183.294815	3491.753802	6.453299	-0.036304	3.236434
183.693374	3499.699709	6.458304	-0.036383	3.239914
183.647532	3507.712421	6.463309	-0.036380	3.243402
184.054954	3515.727354	6.468314	-0.036461	3.246905
184.424503	3523.709334	6.473318	-0.036535	3.250389
184.590132	3531.805034	6.478323	-0.036571	3.253910
184.561155	3539.861054	6.483328	-0.036571	3.257402
184.692347	3547.881582	6.488333	-0.036601	3.260882
184.947169	3555.898810	6.493338	-0.036653	3.264361
185.107621	3563.916645	6.498342	-0.036688	3.267833
185.367989	3571.984707	6.503347	-0.036742	3.271326
185.267919	3580.045497	6.508352	-0.036729	3.274799
185.433942	3588.047371	6.513357	-0.036765	3.278254
185.963618	3596.039649	6.518362	-0.036869	3.281714
186.164350	3604.012692	6.523366	-0.036911	3.285150
186.399274	3612.074767	6.528371	-0.036960	3.288621
186.785836	3620.113763	6.533376	-0.037038	3.292085
186.943957	3628.157692	6.538381	-0.037072	3.295539
187.220735	3636.193045	6.543386	-0.037129	3.298990
187.013956	3644.239611	6.548390	-0.037096	3.302423
187.647913	3652.232589	6.553395	-0.037219	3.305862
188.025490	3660.248761	6.558400	-0.037295	3.309298
188.169566	3668.315975	6.563405	-0.037327	3.312742
188.197781	3676.409168	6.568410	-0.037337	3.316190
188.610641	3684.325875	6.573414	-0.037419	3.319574
188.816481	3692.377726	6.578419	-0.037463	3.323004
189.079744	3700.396946	6.583424	-0.037517	3.326418
189.700072	3708.380221	6.588429	-0.037638	3.329827
189.985997	3716.448192	6.593434	-0.037696	3.333256
189.755034	3724.540596	6.598438	-0.037658	3.336673
190.234798	3732.508124	6.603443	-0.037753	3.340059
190.582226	3740.530140	6.608448	-0.037823	3.343460
190.662030	3748.554647	6.613453	-0.037843	3.346849
191.103222	3756.603004	6.618458	-0.037930	3.350258
191.384232	3764.637887	6.623462	-0.037988	3.353652
191.549691	3772.696118	6.628467	-0.038024	3.357047
191.847385	3780.698553	6.633472	-0.038085	3.360421
192.187947	3788.706279	6.638477	-0.038153	3.363795
192.419133	3796.743409	6.643482	-0.038202	3.367174
192.382702	3804.762173	6.648486	-0.038200	3.370532
192.918527	3812.835384	6.653491	-0.038305	3.373930
193.088302	3820.869394	6.658496	-0.038342	3.377295
193.251623	3828.864937	6.663501	-0.038378	3.380641
193.620004	3836.873748	6.668506	-0.038451	3.383996
193.603219	3844.964117	6.673510	-0.038453	3.387368
194.025866	3852.966625	6.678515	-0.038537	3.390715
194.268121	3861.082360	6.683520	-0.038588	3.394100
194.337578	3869.113955	6.688525	-0.038606	3.397441
194.778243	3877.088132	6.693530	-0.038693	3.400767
194.768101	3885.028532	6.698534	-0.038696	3.404060
195.424820	3893.018859	6.703539	-0.038824	3.407394
195.671123	3901.085803	6.708544	-0.038875	3.410742
195.852247	3909.107239	6.713549	-0.038914	3.414066
196.207041	3917.169235	6.718554	-0.038985	3.417409
196.267980	3925.190658	6.723558	-0.039002	3.420722
196.594644	3933.202028	6.728563	-0.039068	3.424036
196.813702	3941.197466	6.733568	-0.039114	3.427338
197.075144	3949.209430	6.738573	-0.039168	3.430644
197.548867	3957.300962	6.743578	-0.039261	3.433987
197.724175	3965.337243	6.748582	-0.039299	3.437293
197.891585	3973.350781	6.753587	-0.039336	3.440587
198.207562	3981.369297	6.758592	-0.039400	3.443885
198.350581	3989.382818	6.763597	-0.039432	3.447172
198.528689	3997.450112	6.768602	-0.039470	3.450479
198.751737	4005.458234	6.773606	-0.039517	3.453760
199.068673	4013.513271	6.778611	-0.039581	3.457060
199.485837	4021.483999	6.783616	-0.039664	3.460325
199.571577	4029.545387	6.788621	-0.039685	3.463614
199.852592	4037.567625	6.793626	-0.039743	3.466890
199.910601	4045.625127	6.798630	-0.039759	3.470170
200.270550	4053.662732	6.803635	-0.039831	3.473448
200.526483	4061.699332	6.808640	-0.039884	3.476720
200.717698	4069.655524	6.813645	-0.039925	3.479954
200.860880	4077.716204	6.818650	-0.039957	3.483225
201.010066	4085.730845	6.823654	-0.039990	3.486475
201.266644	4093.713829	6.828659	-0.040042	3.489713
201.610853	4101.772537	6.833664	-0.040112	3.492981
201.744841	4109.802577	6.838669	-0.040142	3.496227
202.179585	4117.765904	6.843674	-0.040228	3.499453
202.266227	4125.823957	6.848678	-0.040250	3.502703
202.404959	4133.872367	6.853683	-0.040281	3.505948
202.775346	4141.888097	6.858688	-0.040355	3.509184
202.900580	4149.923085	6.863693	-0.040383	3.512418
203.162911	4157.969127	6.868698	-0.040437	3.515656
203.246940	4165.946690	6.873702	-0.040458	3.518859
203.660989	4173.954160	6.878707	-0.040541	3.522081
203.865940	4182.013006	6.883712	-0.040584	3.525314
204.090306	4190.011528	6.888717	-0.040631	3.528521
204.284199	4198.119750	6.893722	-0.040672	3.531767
204.373542	4206.113507	6.898726	-0.040694	3.534962
204.869291	4214.131982	6.903731	-0.040792	3.538176
205.154282	4222.182284	6.908736	-0.040850	3.541393
205.409216	4230.141097	6.913741	-0.040903	3.544570
205.462631	4238.246125	6.918746	-0.040918	3.547796
205.746250	4246.250423	6.923750	-0.040976	3.550986
206.094069	4254.385525	6.928755	-0.041046	3.554227
206.282292	4262.376989	6.933760	-0.041086	3.557404
206.400319	4270.360342	6.938765	-0.041113	3.560572
206.866580	4278.315974	6.943770	-0.041205	3.563736
206.930504	4286.345296	6.948774	-0.041223	3.566916
207.264214	4294.364593	6.953779	-0.041290	3.570096
207.677388	4302.401258	6.958784	-0.041372	3.573282
207.805546	4310.446888	6.963789	-0.041401	3.576461
208.015166	4318.432878	6.968794	-0.041445	3.579616
207.903357	4326.494301	6.973798	-0.041430	3.582788
208.158549	4334.510343	6.978803	-0.041483	3.585950
208.497815	4342.502955	6.983808	-0.041551	3.589103
208.758950	4350.505143	6.988813	-0.041605	3.592254
209.227796	4358.564174	6.993818	-0.041697	3.595431
209.323775	4366.529556	6.998822	-0.041720	3.598558
209.520931	4374.611138	7.003827	-0.041762	3.601730
209.637540	4382.617862	7.008832	-0.041789	3.604868
209.820301	4390.631766	7.013837	-0.041829	3.608008
210.084578	4398.675798	7.018842	-0.041883	3.611159
210.164547	4406.716666	7.023846	-0.041903	3.614301
210.645748	4414.730211	7.028851	-0.041998	3.617440
210.718206	4422.791364	7.033856	-0.042017	3.620584
211.096853	4430.752538	7.038861	-0.042092	3.623695
211.182458	4438.848535	7.043866	-0.042114	3.626848
211.313359	4446.844064	7.048870	-0.042143	3.629960
211.703555	4454.866498	7.053875	-0.042221	3.633086
212.109103	4462.926362	7.058880	-0.042302	3.636225
212.387681	4470.881233	7.063885	-0.042359	3.639317
212.643078	4478.921165	7.068890	-0.042412	3.642439
212.759064	4486.907389	7.073894	-0.042439	3.645534
213.037639	4494.941937	7.078899	-0.042496	3.648648
213.107164	4503.036395	7.083904	-0.042514	3.651778
213.171138	4511.029004	7.088909	-0.042531	3.654866
213.557859	4519.097420	7.093914	-0.042608	3.657988
213.687141	4527.079939	7.098918	-0.042638	3.661069
213.958946	4535.072710	7.103923	-0.042693	3.664154
214.281488	4543.112802	7.108928	-0.042759	3.667256
214.368124	4551.157632	7.113933	-0.042780	3.670351
214.762083	4559.193850	7.118938	-0.042859	3.673448
214.955232	4567.215285	7.123942	-0.042900	3.676532
215.344100	4575.160636	7.128947	-0.042977	3.679588
215.387326	4583.246291	7.133952	-0.042991	3.682688
215.313570	4591.266479	7.138957	-0.042982	3.685756
215.888254	4599.285366	7.143962	-0.043094	3.688838
216.208270	4607.295079	7.148966	-0.043159	3.691907
216.304278	4615.345745	7.153971	-0.043182	3.694984
216.669680	4623.352216	7.158976	-0.043256	3.698048
216.522780	4631.387005	7.163981	-0.043234	3.701107
216.783748	4639.388270	7.168986	-0.043287	3.704162
216.887479	4647.410426	7.173990	-0.043312	3.707217
217.476058	4655.411614	7.178995	-0.043427	3.710274
217.569754	4663.561285	7.184000	-0.043449	3.713373
217.737786	4671.588054	7.189005	-0.043486	3.716425
217.898304	4679.568460	7.194010	-0.043521	3.719456
218.098873	4687.543043	7.199014	-0.043564	3.722483
218.260458	4695.548104	7.204019	-0.043599	3.725519
218.509833	4703.598021	7.209024	-0.043651	3.728571
218.559328	4711.621693	7.214029	-0.043665	3.731606
219.004537	4719.633922	7.219034	-0.043753	3.734643
219.271278	4727.595272	7.224038	-0.043808	3.737655
219.495578	4735.638662	7.229043	-0.043855	3.740694
219.732470	4743.662232	7.234048	-0.043904	3.743723
219.768794	4751.683996	7.239053	-0.043916	3.746744
220.060285	4759.744783	7.244058	-0.043976	3.749784
220.305793	4767.761882	7.249062	-0.044027	3.752804
220.456804	4775.831213	7.254067	-0.044060	3.755838
220.778406	4783.814419	7.259072	-0.044125	3.758842
221.089564	4791.794797	7.264077	-0.044188	3.761842
221.184594	4799.848052	7.269082	-0.044211	3.764862
221.203181	4807.877379	7.274086	-0.044220	3.767869
221.500366	4815.913157	7.279091	-0.044281	3.770882
221.897862	4823.934477	7.284096	-0.044360	3.773889
221.949486	4831.948661	7.289101	-0.044375	3.776884
222.252629	4839.981108	7.294106	-0.044436	3.779888
222.475683	4847.991317	7.299110	-0.044483	3.782880
222.562042	4855.991714	7.304115	-0.044504	3.785863
222.690408	4864.056397	7.309120	-0.044534	3.788869
222.900419	4872.058131	7.314125	-0.044578	3.791851
223.248515	4880.128790	7.319130	-0.044648	3.794858
223.511813	4888.100788	7.324134	-0.044702	3.797825
223.729358	4896.112925	7.329139	-0.044748	3.800804
223.968059	4904.091490	7.334144	-0.044798	3.803768
224.155659	4912.156024	7.339149	-0.044838	3.806760
224.342022	4920.132593	7.344154	-0.044878	3.809717
224.570544	4928.205055	7.349158	-0.044925	3.812709
224.756956	4936.234826	7.354163	-0.044965	3.815681
225.085464	4944.235834	7.359168	-0.045032	3.818644
225.086200	4952.253267	7.364173	-0.045037	3.821603
225.353564	4960.261060	7.369178	-0.045092	3.824562
225.610859	4968.263879	7.374182	-0.045145	3.827517
225.836570	4976.330744	7.379187	-0.045193	3.830492
226.160708	4984.360307	7.384192	-0.045258	3.833453
226.338179	4992.384834	7.389197	-0.045296	3.836407
226.251897	5000.398770	7.394202	-0.045286	3.839350
226.564647	5008.395972	7.399206	-0.045349	3.842292
226.911875	5016.370308	7.404211	-0.045419	3.845224
227.142450	5024.439925	7.409216	-0.045467	3.848187
227.254155	5032.466924	7.414221	-0.045493	3.851129
227.481480	5040.514316	7.419226	-0.045541	3.854079
227.729577	5048.502800	7.424230	-0.045592	3.857005
227.854148	5056.528917	7.429235	-0.045620	3.859940
228.227188	5064.553835	7.434240	-0.045695	3.862878
228.133760	5072.550950	7.439245	-0.045683	3.865794
228.458786	5080.633682	7.444250	-0.045749	3.868747
228.889462	5088.658824	7.449254	-0.045834	3.871679
229.092001	5096.901382	7.454259	-0.045877	3.874683
229.306894	5104.840666	7.459264	-0.045922	3.877575
229.358737	5112.755021	7.464269	-0.045937	3.880452
229.678107	5120.761879	7.469274	-0.046002	3.883366
229.407929	5128.793612	7.474278	-0.045957	3.886276
229.880992	5136.766779	7.479283	-0.046050	3.889176
230.435170	5144.791036	7.484288	-0.046159	3.892095
230.198739	5152.858902	7.489293	-0.046120	3.895012
230.555424	5160.840951	7.494298	-0.046191	3.897906
230.719606	5168.822537	7.499302	-0.046227	3.900795
231.006960	5176.837550	7.504307	-0.046286	3.903696
231.299371	5184.897330	7.509312	-0.046346	3.906611
231.328671	5192.867492	7.514317	-0.046356	3.909487
231.565798	5200.943965	7.519322	-0.046406	3.912402
231.781947	5208.980805	7.524326	-0.046451	3.915301
231.893265	5216.976015	7.529331	-0.046477	3.918181
232.342426	5224.959461	7.534336	-0.046566	3.921060
232.553378	5232.924298	7.539341	-0.046610	3.923927
232.780701	5241.039478	7.544346	-0.046658	3.926845
232.960130	5248.983878	7.549350	-0.046697	3.929699
233.103484	5257.070030	7.554355	-0.046729	3.932601
233.072457	5265.090556	7.559360	-0.046728	3.935475
233.274226	5273.059386	7.564365	-0.046771	3.938332
233.596294	5281.081512	7.569370	-0.046836	3.941208
233.794261	5289.088552	7.574374	-0.046878	3.944074
233.819760	5297.149133	7.579379	-0.046888	3.946954
234.060728	5305.168568	7.584384	-0.046938	3.949822
234.328344	5313.186542	7.589389	-0.046993	3.952687
234.712980	5321.229431	7.594394	-0.047070	3.955561
234.757802	5329.255829	7.599398	-0.047084	3.958421
234.846640	5337.251770	7.604403	-0.047105	3.961269
235.152267	5345.255640	7.609408	-0.047167	3.964121
235.330553	5353.279263	7.614413	-0.047206	3.966976
235.767229	5361.266845	7.619418	-0.047292	3.969820
235.707330	5369.347566	7.624422	-0.047287	3.972688
235.797602	5377.390203	7.629427	-0.047309	3.975542
235.928038	5385.387478	7.634432	-0.047338	3.978378
236.145184	5393.371571	7.639437	-0.047384	3.981210
236.274580	5401.411325	7.644442	-0.047413	3.984057
236.479487	5409.434045	7.649446	-0.047456	3.986898
236.610236	5417.461508	7.654451	-0.047486	3.989737
236.937388	5425.513346	7.659456	-0.047552	3.992586
236.936282	5433.525582	7.664461	-0.047557	3.995414
237.185019	5441.548319	7.669466	-0.047609	3.998247
237.148847	5449.556697	7.674470	-0.047607	4.001068
237.415419	5457.536077	7.679475	-0.047662	4.003883
237.777665	5465.583548	7.684480	-0.047735	4.006720
237.927422	5473.569801	7.689485	-0.047768	4.009531
237.893404	5481.658603	7.694490	-0.047767	4.012373
238.084679	5489.698901	7.699494	-0.047808	4.015199
238.300150	5497.660249	7.704499	-0.047853	4.017996
238.606490	5505.699933	7.709504	-0.047915	4.020820
238.789607	5513.660657	7.714509	-0.047954	4.023612
239.018529	5521.753477	7.719514	-0.048002	4.026450
239.209027	5529.776089	7.724518	-0.048043	4.029260
239.191540	5537.820303	7.729523	-0.048045	4.032072
239.659847	5545.887287	7.734528	-0.048138	4.034898
239.274463	5553.884883	7.739533	-0.048071	4.037685
239.826465	5561.812184	7.744538	-0.048179	4.040459
239.894847	5569.821609	7.749542	-0.048197	4.043253
240.189273	5577.837159	7.754547	-0.048257	4.046051
240.495143	5585.883929	7.759552	-0.048319	4.048857
240.394598	5593.863244	7.764557	-0.048306	4.051632
240.925821	5601.881627	7.769562	-0.048410	4.054428
241.186958	5609.954433	7.774566	-0.048464	4.057237
241.466504	5617.894606	7.779571	-0.048521	4.059998
241.855015	5625.945750	7.784576	-0.048598	4.062797
242.100293	5633.946174	7.789581	-0.048649	4.065575
242.246971	5642.011063	7.794586	-0.048682	4.068371
242.318977	5650.017773	7.799590	-0.048700	4.071145
242.421312	5658.072112	7.804595	-0.048725	4.073933
242.780097	5666.083181	7.809600	-0.048797	4.076709
242.652018	5674.069964	7.814605	-0.048778	4.079467
243.020407	5682.099000	7.819610	-0.048852	4.082245
243.248373	5690.082954	7.824614	-0.048900	4.085003
243.312190	5698.146602	7.829619	-0.048917	4.087785
243.529960	5706.131988	7.834624	-0.048963	4.090539
243.966913	5714.122722	7.839629	-0.049049	4.093297
244.306284	5722.216177	7.844634	-0.049118	4.096087
244.388202	5730.183280	7.849638	-0.049138	4.098828
244.620187	5738.216501	7.854643	-0.049186	4.101592
245.081740	5746.222189	7.859648	-0.049278	4.104347
245.103685	5754.250568	7.864653	-0.049287	4.107103
245.403549	5762.246853	7.869658	-0.049348	4.109850
245.711114	5770.325786	7.874662	-0.049410	4.112623
245.734433	5778.350408	7.879667	-0.049420	4.115372
245.831839	5786.406026	7.884672	-0.049443	4.118130
245.878676	5794.373042	7.889677	-0.049457	4.120856
246.279814	5802.379314	7.894682	-0.049537	4.123598
246.220069	5810.393727	7.899686	-0.049531	4.126335
246.480499	5818.421359	7.904691	-0.049585	4.129078
246.896413	5826.487440	7.909696	-0.049668	4.131835
246.885942	5834.473198	7.914701	-0.049671	4.134557
247.446363	5842.517752	7.919706	-0.049781	4.137305
247.310794	5850.511179	7.924710	-0.049761	4.140025
247.619283	5858.550575	7.929715	-0.049823	4.142764
247.792343	5866.525647	7.934720	-0.049861	4.145477
248.122672	5874.508044	7.939725	-0.049927	4.148193
248.121903	5882.610906	7.944730	-0.049933	4.150945
248.270389	5890.713230	7.949734	-0.049965	4.153696
248.671565	5898.648649	7.954739	-0.050045	4.156392
249.079959	5906.617721	7.959744	-0.050127	4.159097
249.088950	5914.656947	7.964749	-0.050133	4.161819
249.266340	5922.614735	7.969754	-0.050172	4.164515
249.539451	5930.694683	7.974758	-0.050228	4.167250
249.633648	5938.671272	7.979763	-0.050251	4.169948
249.955370	5946.747465	7.984768	-0.050316	4.172679
250.015760	5954.727339	7.989773	-0.050332	4.175373
250.144524	5962.812993	7.994778	-0.050361	4.178102
250.317372	5970.788655	7.999782	-0.050399	4.180793
250.575650	5978.765002	8.004787	-0.050452	4.183483
250.874315	5986.841810	8.009792	-0.050513	4.186205
250.898668	5994.848030	8.014797	-0.050523	4.188899
251.193417	6002.876183	8.019802	-0.050583	4.191601
251.476557	6010.972272	8.024806	-0.050641	4.194325
251.713582	6018.950525	8.029811	-0.050690	4.197006
251.779377	6026.913092	8.034816	-0.050708	4.199679
251.715316	6034.970330	8.039821	-0.050701	4.202380
252.569638	6042.855366	8.044826	-0.050865	4.205032
252.458215	6050.941205	8.049830	-0.050850	4.207739
252.403361	6058.920453	8.054835	-0.050845	4.210409
252.688539	6067.055412	8.059840	-0.050903	4.213133
252.959514	6075.019602	8.064845	-0.050959	4.215798
252.884700	6083.057800	8.069850	-0.050950	4.218483
252.852104	6091.069955	8.074854	-0.050949	4.221157
253.183444	6098.972951	8.079859	-0.051016	4.223797
253.340235	6107.037688	8.084864	-0.051050	4.226488
253.738894	6115.040880	8.089869	-0.051130	4.229158
254.046183	6123.101548	8.094874	-0.051192	4.231845
254.318036	6131.144054	8.099878	-0.051248	4.234524
254.346836	6139.167447	8.104883	-0.051259	4.237193
254.764910	6147.117670	8.109888	-0.051342	4.239839
254.758110	6155.155035	8.114893	-0.051346	4.242509
254.789834	6163.158802	8.119898	-0.051357	4.245166
254.947974	6171.204717	8.124902	-0.051392	4.247837
255.241772	6179.212619	8.129907	-0.051452	4.250494
255.446012	6187.306244	8.134912	-0.051495	4.253177
255.555580	6195.269833	8.139917	-0.051520	4.255815
255.711404	6203.296677	8.144922	-0.051555	4.258473
255.888818	6211.322386	8.149926	-0.051593	4.261128
255.827322	6219.320519	8.154931	-0.051587	4.263771
256.178675	6227.314115	8.159936	-0.051657	4.266414
256.398344	6235.355857	8.164941	-0.051703	4.269070
256.537578	6243.421746	8.169946	-0.051735	4.271732
256.804735	6251.488629	8.174950	-0.051790	4.274394
257.036870	6259.479043	8.179955	-0.051838	4.277028
257.081302	6267.444896	8.184960	-0.051852	4.279651
257.081909	6275.484102	8.189965	-0.051857	4.282296
257.408001	6283.464483	8.194970	-0.051923	4.284923
257.588787	6291.507508	8.199974	-0.051962	4.287568
257.821277	6299.508724	8.204979	-0.052010	4.290197
258.268909	6307.569884	8.209984	-0.052099	4.292847
258.391768	6315.576117	8.214989	-0.052127	4.295474
258.650987	6323.628010	8.219994	-0.052180	4.298115
258.508611	6331.590182	8.224998	-0.052159	4.300723
259.009733	6339.600838	8.230003	-0.052258	4.303350
259.133048	6347.604029	8.235008	-0.052286	4.305969
259.203518	6355.630510	8.240013	-0.052304	4.308594
259.515030	6363.674797	8.245018	-0.052367	4.311226
259.801448	6371.695037	8.250022	-0.052426	4.313847
259.852406	6379.734914	8.255027	-0.052441	4.316472
260.316220	6387.701024	8.260032	-0.052532	4.319074
260.413948	6395.694235	8.265037	-0.052556	4.321680
260.639321	6403.715528	8.270042	-0.052603	4.324295
260.786526	6411.772168	8.275046	-0.052635	4.326920
260.967378	6419.743826	8.280051	-0.052674	4.329515
261.218448	6427.811104	8.285056	-0.052726	4.332140
261.118880	6435.848171	8.290061	-0.052713	4.334752
261.293035	6443.847097	8.295066	-0.052751	4.337351
261.443735	6451.840781	8.300070	-0.052784	4.339947
261.732624	6459.799076	8.305075	-0.052843	4.342531
261.988350	6467.815850	8.310080	-0.052896	4.345132
262.278036	6475.890859	8.315085	-0.052955	4.347750
262.587086	6483.897204	8.320090	-0.053018	4.350345
262.604390	6492.016219	8.325094	-0.053026	4.352973
262.747411	6500.055752	8.330099	-0.053058	4.355574
263.033217	6508.071449	8.335104	-0.053117	4.358167
263.084178	6515.983211	8.340109	-0.053131	4.360723
263.430810	6523.970738	8.345114	-0.053201	4.363304
263.911810	6531.996562	8.350118	-0.053296	4.365897
263.849007	6539.986565	8.355123	-0.053289	4.368473
264.040604	6548.032074	8.360128	-0.053330	4.371067
264.267331	6556.055666	8.365133	-0.053378	4.373653
264.326552	6564.115085	8.370138	-0.053394	4.376247
264.585076	6572.058515	8.375142	-0.053447	4.378804
264.722471	6580.096126	8.380147	-0.053478	4.381389
265.170307	6588.106242	8.385152	-0.053567	4.383966
265.217683	6596.136500	8.390157	-0.053581	4.386545
265.273324	6604.155811	8.395162	-0.053596	4.389119
265.520112	6612.173915	8.400166	-0.053647	4.391692
265.581998	6620.227968	8.405171	-0.053664	4.394274
265.821938	6628.293792	8.410176	-0.053714	4.396859
265.993387	6636.220188	8.415181	-0.053751	4.399398
266.340786	6644.257893	8.420186	-0.053821	4.401972
266.489478	6652.234068	8.425190	-0.053854	4.404524
266.502357	6660.299972	8.430195	-0.053862	4.407102
266.936210	6668.270682	8.435200	-0.053948	4.409650
266.857433	6676.348370	8.440205	-0.053938	4.412228
267.071942	6684.397276	8.445210	-0.053983	4.414798
267.347319	6692.383527	8.450214	-0.054040	4.417345
267.490750	6700.342991	8.455219	-0.054072	4.419883
267.516948	6708.436133	8.460224	-0.054082	4.422460
267.562420	6716.381697	8.465229	-0.054096	4.424990
267.817009	6724.439042	8.470234	-0.054148	4.427554
267.928525	6732.445060	8.475238	-0.054174	4.430100
267.804048	6740.525554	8.480243	-0.054156	4.432668
268.350277	6748.530540	8.485248	-0.054263	4.435212
268.547290	6756.540702	8.490253	-0.054305	4.437755
268.705003	6764.521562	8.495258	-0.054340	4.440287
269.254694	6772.547703	8.500262	-0.054447	4.442834
269.397161	6780.513457	8.505267	-0.054479	4.445358
269.550602	6788.606951	8.510272	-0.054513	4.447922
269.605642	6796.543479	8.515277	-0.054528	4.450434
270.146814	6804.593655	8.520282	-0.054634	4.452982
270.322489	6812.607207	8.525286	-0.054672	4.455516
270.544339	6820.639731	8.530291	-0.054719	4.458054
270.694219	6828.657905	8.535296	-0.054752	4.460587
270.705125	6836.651459	8.540301	-0.054759	4.463109
271.065849	6844.684625	8.545306	-0.054832	4.465644
271.262881	6852.704316	8.550310	-0.054873	4.468173
271.410864	6860.703339	8.555315	-0.054906	4.470693
271.668975	6868.772348	8.560320	-0.054960	4.473234
271.742919	6876.764410	8.565325	-0.054979	4.475749
271.959797	6884.742819	8.570330	-0.055024	4.478259
271.822723	6892.814405	8.575335	-0.055004	4.480796
271.867428	6900.739813	8.580339	-0.055017	4.483286
272.360642	6908.809053	8.585344	-0.055114	4.485820
272.552711	6916.816903	8.590349	-0.055155	4.488333
272.564378	6924.862661	8.595354	-0.055163	4.490857
272.639513	6932.873593	8.600359	-0.055182	4.493368
272.892572	6940.866729	8.605363	-0.055234	4.495872
273.071308	6948.903893	8.610368	-0.055273	4.498389
273.306341	6956.897317	8.615373	-0.055322	4.500890
273.669313	6964.872401	8.620378	-0.055395	4.503385
273.601792	6972.915011	8.625383	-0.055387	4.505899
273.712273	6980.939892	8.630387	-0.055413	4.508406
274.119252	6989.006354	8.635392	-0.055494	4.510925
274.242736	6997.036266	8.640397	-0.055522	4.513431
274.127161	7005.088197	8.645402	-0.055506	4.515941
274.455713	7013.061755	8.650407	-0.055572	4.518427
274.798789	7020.972586	8.655411	-0.055642	4.520892
274.930665	7029.022471	8.660416	-0.055671	4.523398
274.994025	7037.022048	8.665421	-0.055688	4.525887
275.317043	7045.034754	8.670426	-0.055754	4.528380
275.234137	7053.094233	8.675431	-0.055744	4.530885
275.403788	7061.092590	8.680435	-0.055780	4.533369
275.883715	7069.133210	8.685440	-0.055875	4.535866
275.970146	7077.105718	8.690445	-0.055896	4.538340
275.951648	7085.161607	8.695450	-0.055898	4.540838
276.104138	7093.167844	8.700455	-0.055932	4.543320
276.438277	7101.124402	8.705459	-0.055999	4.545785
276.823887	7109.218377	8.710464	-0.056076	4.548292
276.758978	7117.203469	8.715469	-0.056069	4.550762
276.765949	7125.258287	8.720474	-0.056076	4.553253
277.025069	7133.308677	8.725479	-0.056129	4.555742
277.078879	7141.282281	8.730483	-0.056144	4.558205
277.481516	7149.264361	8.735488	-0.056225	4.560670
277.620568	7157.284966	8.740493	-0.056256	4.563145
277.725823	7165.290827	8.745498	-0.056281	4.565614
278.055506	7173.322898	8.750503	-0.056347	4.568090
278.215144	7181.292879	8.755507	-0.056382	4.570546
278.511210	7189.393766	8.760512	-0.056443	4.573040
278.551778	7197.393025	8.765517	-0.056455	4.575502
278.878124	7205.420621	8.770522	-0.056521	4.577971
279.029893	7213.408175	8.775527	-0.056555	4.580427
279.163307	7221.400099	8.780531	-0.056585	4.582882
279.319759	7229.442117	8.785536	-0.056619	4.585352
279.526281	7237.437640	8.790541	-0.056663	4.587805
279.673892	7245.475218	8.795546	-0.056696	4.590271
279.777724	7253.588492	8.800551	-0.056720	4.592758
279.868666	7261.559448	8.805555	-0.056742	4.595201
279.823864	7269.645798	8.810560	-0.056739	4.597677
279.900413	7277.522300	8.815565	-0.056759	4.600088
279.878068	7285.607066	8.820570	-0.056760	4.602561
280.032111	7293.528833	8.825575	-0.056794	4.604983
280.306229	7301.553071	8.830579	-0.056850	4.607435
280.344951	7309.623319	8.835584	-0.056862	4.609900
280.810775	7317.636138	8.840589	-0.056954	4.612346
280.843448	7325.638344	8.845594	-0.056966	4.614787
280.907576	7333.732940	8.850599	-0.056983	4.617255
280.982421	7341.654658	8.855603	-0.057002	4.619670
280.989529	7349.752635	8.860608	-0.057008	4.622136
281.163931	7357.651238	8.865613	-0.057046	4.624541
281.421795	7365.730770	8.870618	-0.057099	4.626999
281.682470	7373.733596	8.875623	-0.057153	4.629433
282.189164	7381.701426	8.880627	-0.057253	4.631854
282.432404	7389.760149	8.885632	-0.057303	4.634302
282.764294	7397.843085	8.890637	-0.057370	4.636756
282.786875	7405.771869	8.895642	-0.057380	4.639162
282.924511	7413.792742	8.900647	-0.057410	4.641595
283.162854	7421.776056	8.905651	-0.057460	4.644015
283.428198	7429.859601	8.910656	-0.057515	4.646464
283.485165	7437.821822	8.915661	-0.057531	4.648875
283.698097	7445.909644	8.920666	-0.057575	4.651322
283.807135	7453.912539	8.925671	-0.057601	4.653743
283.837624	7461.917190	8.930675	-0.057612	4.656163
284.438977	7469.936239	8.935680	-0.057729	4.658586
284.683161	7477.935023	8.940685	-0.057780	4.661001
284.495446	7485.924256	8.945690	-0.057750	4.663413
284.586015	7494.001978	8.950695	-0.057772	4.665850
284.939072	7501.942636	8.955699	-0.057843	4.668244
285.100796	7510.012732	8.960704	-0.057878	4.670676
285.198137	7518.086694	8.965709	-0.057902	4.673108
285.376912	7526.098027	8.970714	-0.057940	4.675520
285.754370	7534.080680	8.975719	-0.058016	4.677921
285.903529	7542.005774	8.980723	-0.058049	4.680305
286.341029	7550.072089	8.985728	-0.058135	4.682729
286.539517	7558.027708	8.990733	-0.058178	4.685119
286.804431	7566.099246	8.995738	-0.058232	4.687542
286.808755	7574.079406	9.000743	-0.058238	4.689937
287.018402	7582.147529	9.005747	-0.058282	4.692357
287.257424	7590.131618	9.010752	-0.058332	4.694750
287.409111	7598.202515	9.015757	-0.058366	4.697169
287.515251	7606.142755	9.020762	-0.058391	4.699547
287.883407	7614.208276	9.025767	-0.058464	4.701960
287.782522	7622.127779	9.030771	-0.058451	4.704330
287.895573	7630.264129	9.035776	-0.058477	4.706763
287.826467	7638.243193	9.040781	-0.058469	4.709148
288.376515	7646.205016	9.045786	-0.058577	4.711525
288.252514	7654.321386	9.050791	-0.058559	4.713949
288.445228	7662.317387	9.055795	-0.058600	4.716335
288.742811	7670.321722	9.060800	-0.058661	4.718722
288.754936	7678.333569	9.065805	-0.058668	4.721111
288.865828	7686.315944	9.070810	-0.058694	4.723489
289.120418	7694.335387	9.075815	-0.058747	4.725877
289.244835	7702.360719	9.080819	-0.058775	4.728265
289.588305	7710.361114	9.085824	-0.058845	4.730645
289.659648	7718.415102	9.090829	-0.058863	4.733040
289.838108	7726.456579	9.095834	-0.058902	4.735429
290.000835	7734.442094	9.100839	-0.058937	4.737801
290.110495	7742.446824	9.105843	-0.058963	4.740177
290.327971	7750.486390	9.110848	-0.059008	4.742563
290.407482	7758.459968	9.115853	-0.059028	4.744927
290.693935	7766.500187	9.120858	-0.059087	4.747310
290.833802	7774.490012	9.125863	-0.059118	4.749677
290.879490	7782.523790	9.130867	-0.059132	4.752057
291.081046	7790.613240	9.135872	-0.059175	4.754451
291.387140	7798.640695	9.140877	-0.059237	4.756824
291.488428	7806.537532	9.145882	-0.059261	4.759159
291.628248	7814.578275	9.150887	-0.059292	4.761536
291.691916	7822.572360	9.155891	-0.059309	4.763897
291.967043	7830.577649	9.160896	-0.059366	4.766260
291.912050	7838.559039	9.165901	-0.059361	4.768616
292.175594	7846.610366	9.170906	-0.059415	4.770990
292.408092	7854.691837	9.175911	-0.059464	4.773371
292.292920	7862.688565	9.180915	-0.059447	4.775729
292.391939	7870.694551	9.185920	-0.059471	4.778086
292.501072	7878.715299	9.190925	-0.059497	4.780447
292.847381	7886.705519	9.195930	-0.059566	4.782797
292.992446	7894.737010	9.200935	-0.059599	4.785158
292.992234	7902.688435	9.205939	-0.059604	4.787496
293.115017	7910.791332	9.210944	-0.059632	4.789876
293.434918	7918.751581	9.215949	-0.059697	4.792212
293.524442	7926.775894	9.220954	-0.059718	4.794567
293.877972	7934.836257	9.225959	-0.059790	4.796930
293.965550	7942.780189	9.230963	-0.059811	4.799259
293.910162	7950.897126	9.235968	-0.059806	4.801638
293.869438	7958.813660	9.240973	-0.059804	4.803958
293.997787	7966.860669	9.245978	-0.059833	4.806313
294.175390	7974.862399	9.250983	-0.059871	4.808654
294.321888	7982.859011	9.255987	-0.059903	4.810992
294.625965	7990.340128	9.260992	-0.059965	4.813178
294.829119	7994.784282	9.265997	-0.060006	4.814476

294.665466	7997.276080	9.271002	-0.059977	4.815205
294.839008	7998.630945	9.276007	-0.060010	4.815600
294.861214	7999.106880	9.281011	-0.060014	4.815739
294.832802	8000.130136	9.286016	-0.060010	4.816038
294.871869	8000.107337	9.291021	-0.060017	4.816031
295.116345	8000.110723	9.296026	-0.060063	4.816031
295.292489	8000.138513	9.301031	-0.060095	4.816038
295.357275	8000.110839	9.306035	-0.060108	4.816030
295.629193	8000.140375	9.311040	-0.060158	4.816037
295.588320	8000.090470	9.316045	-0.060151	4.816022
295.646130	8000.079767	9.321050	-0.060161	4.816019
295.897903	8000.116418	9.326055	-0.060208	4.816028
295.885708	8000.054210	9.331059	-0.060206	4.816010
296.014585	8000.105720	9.336064	-0.060230	4.816025
295.829616	8000.124791	9.341069	-0.060195	4.816031
296.088765	8000.082492	9.346074	-0.060244	4.816017
296.326404	8000.138123	9.351079	-0.060288	4.816032
296.174019	8000.128932	9.356083	-0.060260	4.816030
296.320160	8000.158315	9.361088	-0.060287	4.816038
296.299530	8000.103433	9.366093	-0.060283	4.816022
296.402281	8000.051870	9.371098	-0.060302	4.816007
296.382504	8000.089984	9.376103	-0.060298	4.816018
296.150410	8000.054760	9.381107	-0.060255	4.816009
296.203029	8000.119842	9.386112	-0.060265	4.816028
296.288551	8000.133157	9.391117	-0.060281	4.816031
296.446421	8000.075118	9.396122	-0.060310	4.816013
296.459798	8000.094599	9.401127	-0.060313	4.816019
296.610190	8000.099478	9.406131	-0.060341	4.816020
296.653041	8000.118428	9.411136	-0.060349	4.816025
296.740109	8000.041998	9.416141	-0.060365	4.816002
296.632808	8000.056073	9.421146	-0.060345	4.816007
296.524876	8000.153497	9.426151	-0.060325	4.816036
296.782985	8000.116522	9.431155	-0.060373	4.816024
296.848904	8000.079250	9.436160	-0.060385	4.816012
296.874137	8000.079710	9.441165	-0.060390	4.816012
296.716198	8000.077898	9.446170	-0.060360	4.816013
296.972515	8000.148834	9.451175	-0.060408	4.816032
296.723378	8000.102610	9.456179	-0.060362	4.816020
296.860134	8000.148922	9.461184	-0.060387	4.816033
296.909280	8000.135925	9.466189	-0.060396	4.816029
296.893948	8000.108926	9.471194	-0.060394	4.816021
297.118047	8000.110876	9.476199	-0.060435	4.816020
296.943690	8000.061740	9.481203	-0.060403	4.816007
297.003177	8000.028625	9.486208	-0.060414	4.815997
296.887624	8000.102398	9.491213	-0.060392	4.816019
296.962473	8000.021470	9.496218	-0.060406	4.815995
297.059510	8000.098052	9.501223	-0.060424	4.816017
296.897294	8000.038450	9.506227	-0.060394	4.816000
297.013088	8000.092930	9.511232	-0.060416	4.816015
297.035435	8000.101887	9.516237	-0.060420	4.816018
297.178399	8000.051057	9.521242	-0.060447	4.816002
297.186102	8000.127078	9.526247	-0.060448	4.816025
297.213138	8000.091234	9.531251	-0.060453	4.816014
297.123625	8000.135558	9.536256	-0.060436	4.816027
297.181132	8000.136606	9.541261	-0.060447	4.816027
297.114287	8000.134318	9.546266	-0.060435	4.816027
297.261169	8000.154097	9.551271	-0.060462	4.816032
297.213271	8000.075205	9.556275	-0.060453	4.816009
297.254042	8000.082361	9.561280	-0.060461	4.816011
297.082226	8000.108083	9.566285	-0.060429	4.816020
297.344239	8000.078662	9.571290	-0.060477	4.816010
297.236063	8000.133333	9.576295	-0.060457	4.816026
297.348186	8000.114002	9.581299	-0.060478	4.816020
297.337166	8000.127695	9.586304	-0.060476	4.816024
297.218268	8000.139420	9.591309	-0.060454	4.816028
297.305975	8000.097201	9.596314	-0.060470	4.816015
297.357146	8000.141953	9.601319	-0.060480	4.816028
297.569886	8000.088121	9.606323	-0.060519	4.816011
297.501772	8000.081534	9.611328	-0.060507	4.816010
297.481613	8000.138879	9.616333	-0.060503	4.816026
297.627171	8000.103059	9.621338	-0.060530	4.816015
297.584015	8000.084103	9.626343	-0.060522	4.816010
297.545260	8000.057746	9.631347	-0.060515	4.816002
297.824053	8000.106650	9.636352	-0.060567	4.816015
297.637867	8000.121423	9.641357	-0.060532	4.816020
297.368028	8000.114363	9.646362	-0.060482	4.816020
297.584604	8000.132207	9.651367	-0.060522	4.816024
297.333226	8000.135103	9.656371	-0.060475	4.816026
297.475756	8000.170834	9.661376	-0.060502	4.816036
297.650825	8000.183647	9.666381	-0.060535	4.816039
297.641242	8000.116140	9.671386	-0.060533	4.816019
297.732086	8000.180854	9.676391	-0.060550	4.816037
297.664443	8000.106944	9.681395	-0.060537	4.816016
297.864523	8000.122350	9.686400	-0.060574	4.816020
297.687315	8000.087055	9.691405	-0.060541	4.816010
297.609797	8000.065334	9.696410	-0.060527	4.816004
297.878059	8000.114047	9.701415	-0.060577	4.816017
297.969921	8000.119998	9.706419	-0.060594	4.816018
297.997799	8000.135469	9.711424	-0.060599	4.816023
297.758703	8000.117213	9.716429	-0.060555	4.816019
297.795851	8000.074071	9.721434	-0.060561	4.816006
297.814373	8000.105403	9.726439	-0.060565	4.816015
297.625706	8000.050661	9.731443	-0.060530	4.816000
297.738473	8000.056993	9.736448	-0.060551	4.816001
297.758832	8000.124696	9.741453	-0.060555	4.816021
297.737573	8000.084764	9.746458	-0.060551	4.816009
297.826796	8000.155861	9.751463	-0.060567	4.816030
297.769352	8000.102444	9.756467	-0.060557	4.816014
297.782923	8000.133686	9.761472	-0.060559	4.816023
297.965795	8000.110303	9.766477	-0.060593	4.816015
298.167758	8000.074443	9.771482	-0.060631	4.816004
298.156427	8000.109505	9.776487	-0.060629	4.816014
297.863695	8000.085996	9.781491	-0.060574	4.816009
298.033799	8000.110474	9.786496	-0.060606	4.816015
298.006750	8000.115324	9.791501	-0.060601	4.816017
297.871240	8000.120333	9.796506	-0.060576	4.816019
298.011711	8000.130377	9.801511	-0.060602	4.816021
297.983184	8000.101000	9.806515	-0.060596	4.816013
297.829942	8000.134542	9.811520	-0.060568	4.816023
297.867360	8000.096749	9.816525	-0.060575	4.816012
298.124144	8000.078990	9.821530	-0.060623	4.816005
298.138565	8000.129485	9.826535	-0.060625	4.816020
298.171450	8000.069165	9.831539	-0.060631	4.816002
298.194703	8000.111271	9.836544	-0.060636	4.816015
298.167261	8000.078707	9.841549	-0.060631	4.816005
298.235849	8000.064996	9.846554	-0.060643	4.816001
298.408628	8000.103418	9.851559	-0.060676	4.816011
298.266778	8000.108311	9.856563	-0.060649	4.816013
298.263314	8000.163824	9.861568	-0.060649	4.816030
298.174935	8000.123735	9.866573	-0.060632	4.816018
298.304366	8000.091896	9.871578	-0.060656	4.816008
298.354916	8000.119538	9.876583	-0.060666	4.816016
298.096752	8000.114827	9.881587	-0.060617	4.816016
298.269128	8000.119041	9.886592	-0.060650	4.816016
298.281752	8000.136372	9.891597	-0.060652	4.816021
298.226875	8000.112926	9.896602	-0.060642	4.816015
298.239514	8000.125982	9.901607	-0.060644	4.816019
298.227367	8000.012470	9.906611	-0.060642	4.815985
298.351323	8000.107715	9.911616	-0.060665	4.816013
298.183296	8000.136712	9.916621	-0.060634	4.816022
298.447295	8000.093434	9.921626	-0.060683	4.816008
298.571390	8000.149137	9.926631	-0.060706	4.816024
298.519106	8000.110776	9.931635	-0.060696	4.816013
298.415530	8000.123849	9.936640	-0.060677	4.816017
298.632099	8000.151314	9.941645	-0.060717	4.816024
298.320737	8000.106087	9.946650	-0.060659	4.816012
298.457006	8000.096817	9.951655	-0.060685	4.816009
298.427813	8000.108041	9.956659	-0.060679	4.816012
298.550987	8000.157315	9.961664	-0.060702	4.816026
298.520016	8000.137511	9.966669	-0.060696	4.816020
298.447404	8000.106261	9.971674	-0.060683	4.816012
298.605599	8000.164724	9.976679	-0.060712	4.816028
298.621835	8000.063486	9.981683	-0.060715	4.815998
298.533673	8000.096078	9.986688	-0.060699	4.816008
298.527690	8000.115207	9.991693	-0.060698	4.816014
298.564411	8000.096639	9.996698	-0.060705	4.816008
298.364383	8000.181697	10.001703	-0.060667	4.816034
298.412960	8000.136626	10.006707	-0.060676	4.816021
298.476866	8000.113210	10.011712	-0.060688	4.816014
298.318942	8000.129566	10.016717	-0.060659	4.816019
298.535137	8000.099310	10.021722	-0.060699	4.816009
298.847110	8000.166993	10.026727	-0.060757	4.816027
298.656257	8000.092970	10.031731	-0.060722	4.816007
298.580232	8000.131128	10.036736	-0.060707	4.816018
298.714050	8000.148532	10.041741	-0.060732	4.816023
298.519634	8000.104371	10.046746	-0.060696	4.816011
298.622386	8000.060288	10.051751	-0.060715	4.815997
298.532514	8000.109950	10.056755	-0.060699	4.816012
298.571544	8000.090355	10.061760	-0.060706	4.816006
298.528444	8000.160108	10.066765	-0.060698	4.816027
298.482976	8000.105839	10.071770	-0.060689	4.816011
298.777270	8000.127241	10.076775	-0.060744	4.816016
298.531883	8000.109938	10.081779	-0.060698	4.816012
298.679761	8000.137218	10.086784	-0.060726	4.816020
298.803115	8000.150157	10.091789	-0.060749	4.816023
298.835551	8000.090897	10.096794	-0.060755	4.816005
298.622903	8000.166106	10.101799	-0.060715	4.816028
298.612122	8000.163772	10.106803	-0.060713	4.816028
298.728410	8000.114592	10.111808	-0.060735	4.816013
298.678387	8000.156431	10.116813	-0.060726	4.816025
298.621227	8000.148975	10.121818	-0.060715	4.816023
298.860478	8000.192886	10.126823	-0.060760	4.816035
298.738878	8000.063481	10.131827	-0.060737	4.815998
298.786628	8000.060077	10.136832	-0.060746	4.815996
298.792887	8000.092255	10.141837	-0.060747	4.816006
298.658791	8000.112252	10.146842	-0.060722	4.816012
298.733980	8000.106143	10.151847	-0.060736	4.816010
298.691573	8000.097887	10.156851	-0.060728	4.816008
298.702502	8000.105568	10.161856	-0.060730	4.816010
298.908562	8000.171318	10.166861	-0.060769	4.816028
298.708492	8000.125984	10.171866	-0.060731	4.816016
298.818362	8000.173947	10.176871	-0.060752	4.816030
298.576448	8000.092580	10.181875	-0.060707	4.816007
298.698892	8000.103364	10.186880	-0.060730	4.816010
298.679104	8000.144686	10.191885	-0.060726	4.816022
298.635573	8000.142822	10.196890	-0.060718	4.816021
298.678429	8000.183150	10.201895	-0.060726	4.816033
298.608544	8000.158361	10.206899	-0.060713	4.816026
298.834903	8000.180661	10.211904	-0.060755	4.816031
298.870933	8000.187731	10.216909	-0.060762	4.816033
298.821624	8000.197519	10.221914	-0.060752	4.816036
298.843425	8000.182954	10.226919	-0.060757	4.816032
298.615043	8000.179855	10.231923	-0.060714	4.816032
298.723087	8000.143350	10.236928	-0.060734	4.816021
298.755007	8000.134313	10.241933	-0.060740	4.816018
298.805470	8000.096758	10.246938	-0.060749	4.816007
298.727600	8000.175496	10.251943	-0.060735	4.816030
298.768797	8000.150597	10.256947	-0.060743	4.816023
298.734301	8000.179893	10.261952	-0.060736	4.816032
298.539313	8000.194504	10.266957	-0.060700	4.816037
298.813694	8000.164241	10.271962	-0.060751	4.816027
298.914118	8000.163936	10.276967	-0.060770	4.816026
298.955791	8000.137977	10.281971	-0.060777	4.816018
298.913915	8000.127593	10.286976	-0.060770	4.816015
298.811842	8000.130006	10.291981	-0.060751	4.816017
298.871422	8000.122543	10.296986	-0.060762	4.816014
298.932428	8000.141825	10.301991	-0.060773	4.816020
298.741092	8000.123370	10.306995	-0.060737	4.816015
298.973293	8000.145777	10.312000	-0.060781	4.816020
299.053550	8000.129073	10.317005	-0.060796	4.816015
298.885701	8000.121734	10.322010	-0.060764	4.816014
298.940465	8000.172967	10.327015	-0.060775	4.816029
298.864391	8000.112795	10.332019	-0.060760	4.816011
298.918967	8000.082796	10.337024	-0.060770	4.816002
299.016558	8000.158323	10.342029	-0.060789	4.816024
299.146049	8000.124348	10.347034	-0.060813	4.816013
299.173224	8000.168664	10.352039	-0.060818	4.816026
299.015996	8000.120905	10.357043	-0.060789	4.816013
299.076437	8000.122008	10.362048	-0.060800	4.816013
298.968433	8000.127518	10.367053	-0.060780	4.816015
299.018309	8000.108121	10.372058	-0.060789	4.816009
299.225398	8000.201680	10.377063	-0.060828	4.816035
299.065533	8000.166698	10.382067	-0.060798	4.816026
298.863557	8000.141636	10.387072	-0.060760	4.816020
298.865089	8000.147008	10.392077	-0.060760	4.816021
299.096455	8000.108478	10.397082	-0.060804	4.816009
299.175975	8000.130237	10.402087	-0.060818	4.816015
298.943129	8000.070410	10.407091	-0.060775	4.815999
299.095291	8000.115938	10.412096	-0.060803	4.816011
298.944920	8000.107850	10.417101	-0.060775	4.816010
298.749250	8000.040152	10.422106	-0.060739	4.815991
298.925200	8000.116040	10.427111	-0.060772	4.816012
298.839324	8000.109129	10.432115	-0.060756	4.816010
298.874504	8000.096945	10.437120	-0.060762	4.816007
298.947167	8000.116441	10.442125	-0.060776	4.816012
298.915261	8000.101964	10.447130	-0.060770	4.816008
299.128128	8000.109055	10.452135	-0.060809	4.816009
298.989351	8000.089422	10.457139	-0.060784	4.816004
298.942576	8000.093912	10.462144	-0.060775	4.816005
298.917616	8000.123383	10.467149	-0.060770	4.816014
298.779444	8000.095210	10.472154	-0.060744	4.816007
299.240458	8000.141032	10.477159	-0.060830	4.816018
299.181565	8000.134613	10.482163	-0.060819	4.816016
299.268592	8000.069935	10.487168	-0.060836	4.815997
299.168140	8000.065964	10.492173	-0.060817	4.815996
299.183836	8000.073732	10.497178	-0.060820	4.815998
299.334206	8000.114953	10.502183	-0.060848	4.816010
299.245060	8000.099432	10.507187	-0.060831	4.816005
299.519808	8000.091621	10.512192	-0.060882	4.816002
299.283149	8000.133260	10.517197	-0.060838	4.816015
299.105990	8000.121476	10.522202	-0.060805	4.816013
299.098573	8000.145923	10.527207	-0.060804	4.816020
299.195090	8000.139134	10.532211	-0.060822	4.816017
299.245935	8000.104791	10.537216	-0.060831	4.816007
299.049200	8000.199530	10.542221	-0.060795	4.816036
299.181629	8000.149576	10.547226	-0.060819	4.816020
299.359269	8000.176332	10.552231	-0.060852	4.816027
299.261740	8000.138212	10.557235	-0.060834	4.816017
299.252726	8000.117740	10.562240	-0.060833	4.816011
299.314375	8000.125278	10.567245	-0.060844	4.816013
299.391436	8000.026218	10.572250	-0.060858	4.815983
299.366303	8000.104850	10.577255	-0.060854	4.816006
299.350047	8000.102416	10.582259	-0.060851	4.816006
299.369438	8000.117733	10.587264	-0.060854	4.816010
299.234466	8000.110994	10.592269	-0.060829	4.816009
299.266955	8000.074179	10.597274	-0.060835	4.815998
299.372012	8000.142362	10.602279	-0.060855	4.816017
299.138399	8000.129547	10.607283	-0.060811	4.816015
299.329108	8000.142647	10.612288	-0.060847	4.816018
299.515588	8000.181322	10.617293	-0.060882	4.816028
299.358178	8000.170967	10.622298	-0.060852	4.816026
299.374170	8000.176603	10.627303	-0.060855	4.816027
299.316531	8000.103941	10.632307	-0.060844	4.816006
299.364940	8000.091998	10.637312	-0.060853	4.816003
299.168900	8000.145067	10.642317	-0.060817	4.816019
299.178025	8000.054385	10.647322	-0.060819	4.815993
299.471998	8000.137773	10.652327	-0.060873	4.816015
299.136498	8000.147681	10.657331	-0.060811	4.816020
299.102275	8000.121405	10.662336	-0.060805	4.816013
299.139030	8000.212924	10.667341	-0.060811	4.816039
299.367492	8000.150829	10.672346	-0.060854	4.816020
299.221080	8000.126780	10.677351	-0.060827	4.816014
299.215547	8000.107440	10.682355	-0.060826	4.816008
299.232010	8000.098122	10.687360	-0.060829	4.816005
299.356491	8000.126045	10.692365	-0.060852	4.816013
299.277411	8000.078643	10.697370	-0.060837	4.815999
299.400563	8000.149294	10.702375	-0.060860	4.816019
299.220002	8000.046600	10.707379	-0.060826	4.815990
299.078915	8000.050438	10.712384	-0.060800	4.815992
299.414780	8000.126040	10.717389	-0.060863	4.816012
299.353668	8000.109961	10.722394	-0.060851	4.816008
299.410950	8000.145208	10.727399	-0.060862	4.816018
299.413975	8000.090754	10.732403	-0.060863	4.816002
299.369026	8000.037563	10.737408	-0.060854	4.815987
299.496246	8000.121113	10.742413	-0.060878	4.816010
299.255721	8000.069696	10.747418	-0.060833	4.815997
299.571044	8000.101102	10.752423	-0.060892	4.816004
299.543070	8000.100592	10.757427	-0.060887	4.816004
299.332937	8000.093550	10.762432	-0.060847	4.816003
299.401648	8000.171758	10.767437	-0.060860	4.816026
299.397630	8000.123588	10.772442	-0.060860	4.816012
299.131907	8000.220274	10.777447	-0.060810	4.816041
299.080020	8000.180850	10.782451	-0.060800	4.816030
299.335267	8000.153445	10.787456	-0.060848	4.816021
299.355466	8000.207254	10.792461	-0.060852	4.816036
299.337780	8000.156697	10.797466	-0.060848	4.816022
299.571587	8000.169515	10.802471	-0.060892	4.816024
299.451345	8000.145944	10.807475	-0.060870	4.816018
299.467034	8000.125923	10.812480	-0.060872	4.816012
299.439967	8000.158562	10.817485	-0.060867	4.816022
299.420579	8000.130419	10.822490	-0.060864	4.816014
299.491356	8000.179807	10.827495	-0.060877	4.816028
299.295829	8000.108903	10.832499	-0.060841	4.816008
299.317322	8000.077231	10.837504	-0.060845	4.815999
299.608342	8000.143465	10.842509	-0.060899	4.816016
299.504687	8000.141573	10.847514	-0.060879	4.816016
299.589206	8000.179455	10.852519	-0.060895	4.816027
299.663269	8000.120954	10.857523	-0.060909	4.816010
299.539000	8000.072727	10.862528	-0.060886	4.815996
299.390987	8000.154460	10.867533	-0.060858	4.816021
299.498626	8000.151081	10.872538	-0.060878	4.816019
299.605895	8000.178691	10.877543	-0.060898	4.816027
299.574853	8000.134303	10.882547	-0.060893	4.816014
299.635410	8000.094793	10.887552	-0.060904	4.816002
299.580424	8000.162193	10.892557	-0.060894	4.816022
299.578090	8000.119398	10.897562	-0.060893	4.816010
299.647366	8000.185860	10.902567	-0.060906	4.816029
299.572943	8000.140680	10.907571	-0.060892	4.816016
299.221673	8000.217635	10.912576	-0.060827	4.816040
299.229541	8000.209228	10.917581	-0.060828	4.816038
299.495266	8000.189496	10.922586	-0.060878	4.816030
299.573980	8000.201621	10.927591	-0.060892	4.816034
299.521165	8000.098051	10.932595	-0.060883	4.816004
299.471175	8000.152716	10.937600	-0.060873	4.816020
299.564130	8000.175790	10.942605	-0.060891	4.816026
299.364759	8000.140086	10.947610	-0.060853	4.816017
299.617019	8000.179961	10.952615	-0.060900	4.816027
299.524876	8000.122701	10.957619	-0.060883	4.816011
299.509619	8000.126698	10.962624	-0.060880	4.816012
299.559476	8000.187461	10.967629	-0.060890	4.816030
299.555802	8000.175637	10.972634	-0.060889	4.816026
299.514720	8000.133203	10.977639	-0.060881	4.816014
299.350647	8000.102419	10.982643	-0.060851	4.816006
299.430934	8000.137018	10.987648	-0.060866	4.816015
299.548521	8000.180848	10.992653	-0.060888	4.816028
299.222474	8000.072291	10.997658	-0.060827	4.815998
299.318669	8000.082597	11.002663	-0.060845	4.816000
299.636803	8000.156808	11.007667	-0.060904	4.816020
299.512497	8000.164158	11.012672	-0.060881	4.816023
299.278439	8000.188743	11.017677	-0.060837	4.816031
299.461738	8000.125823	11.022682	-0.060871	4.816012
299.432803	8000.153083	11.027687	-0.060866	4.816020
299.176840	8000.148411	11.032691	-0.060818	4.816020
299.391882	8000.103171	11.037696	-0.060858	4.816006
299.587778	8000.086440	11.042701	-0.060895	4.816000
299.436718	8000.058031	11.047706	-0.060867	4.815992
299.638995	8000.119439	11.052711	-0.060904	4.816009
299.424393	8000.079182	11.057715	-0.060864	4.815999
299.420150	8000.087655	11.062720	-0.060864	4.816001
299.501088	8000.130815	11.067725	-0.060879	4.816013
299.454901	8000.124628	11.072730	-0.060870	4.816012
299.776103	8000.197827	11.077735	-0.060930	4.816031
299.359087	8000.121810	11.082739	-0.060852	4.816011
299.666326	8000.119937	11.087744	-0.060910	4.816009
299.768629	8000.106841	11.092749	-0.060929	4.816005
299.590122	8000.083275	11.097754	-0.060895	4.815999
299.548583	8000.133819	11.102759	-0.060888	4.816014
299.593145	8000.128220	11.107763	-0.060896	4.816012
299.456882	8000.131076	11.112768	-0.060871	4.816014
299.231704	8000.185750	11.117773	-0.060829	4.816031
299.423281	8000.130463	11.122778	-0.060864	4.816014
299.726718	8000.144552	11.127783	-0.060921	4.816016
299.588727	8000.124932	11.132787	-0.060895	4.816011
299.632675	8000.137491	11.137792	-0.060903	4.816015
299.623320	8000.199312	11.142797	-0.060902	4.816033
299.421480	8000.173182	11.147802	-0.060864	4.816026
299.361924	8000.153925	11.152807	-0.060853	4.816021
299.268392	8000.134048	11.157811	-0.060835	4.816015
299.302064	8000.156038	11.162816	-0.060842	4.816022
299.160094	8000.180167	11.167821	-0.060815	4.816030
299.234976	8000.156951	11.172826	-0.060829	4.816022
299.454603	8000.224020	11.177831	-0.060870	4.816041
299.208763	8000.201362	11.182835	-0.060824	4.816035
299.302118	8000.169933	11.187840	-0.060842	4.816026
299.469561	8000.206123	11.192845	-0.060873	4.816035
299.487076	8000.173309	11.197850	-0.060876	4.816026
299.367325	8000.189293	11.202855	-0.060854	4.816031
299.000401	8000.232829	11.207859	-0.060786	4.816046
299.475051	8000.154920	11.212864	-0.060874	4.816020
299.414916	8000.196574	11.217869	-0.060863	4.816033
299.289806	8000.111993	11.222874	-0.060839	4.816009
299.446695	8000.214255	11.227879	-0.060869	4.816038
299.429406	8000.155155	11.232883	-0.060865	4.816021
299.523775	8000.170772	11.237888	-0.060883	4.816025
299.610832	8000.187325	11.242893	-0.060899	4.816029
299.470902	8000.167669	11.247898	-0.060873	4.816024
299.570443	8000.187656	11.252903	-0.060892	4.816030
299.433188	8000.144536	11.257907	-0.060866	4.816018
299.263184	8000.214111	11.262912	-0.060834	4.816039
299.222266	8000.199470	11.267917	-0.060827	4.816035
299.169118	8000.168573	11.272922	-0.060817	4.816026
299.649353	8000.149550	11.277927	-0.060906	4.816018
299.705852	8000.093935	11.282931	-0.060917	4.816001
299.781472	8000.107072	11.287936	-0.060931	4.816005
299.844061	8000.093251	11.292941	-0.060943	4.816000
299.783615	8000.096423	11.297946	-0.060931	4.816002
299.604244	8000.162621	11.302951	-0.060898	4.816022
299.678329	8000.142597	11.307955	-0.060912	4.816016
299.690283	8000.149228	11.312960	-0.060914	4.816018
299.517203	8000.169582	11.317965	-0.060882	4.816025
299.578703	8000.137572	11.322970	-0.060893	4.816015
299.904557	8000.176654	11.327975	-0.060954	4.816025
299.597286	8000.145392	11.332979	-0.060897	4.816017
299.632814	8000.108633	11.337984	-0.060903	4.816006
299.771216	8000.156049	11.342989	-0.060929	4.816019
299.575913	8000.125763	11.347994	-0.060893	4.816011
299.622986	8000.098834	11.352999	-0.060901	4.816003
299.586798	8000.124893	11.358003	-0.060895	4.816011
299.669603	8000.113579	11.363008	-0.060910	4.816007
299.674993	8000.176737	11.368013	-0.060911	4.816026
299.640381	8000.141903	11.373018	-0.060905	4.816016
299.703374	8000.199700	11.378023	-0.060916	4.816032
299.834651	8000.187133	11.383027	-0.060941	4.816028
299.807995	8000.169546	11.388032	-0.060936	4.816023
299.716599	8000.182840	11.393037	-0.060919	4.816027
299.674098	8000.104041	11.398042	-0.060911	4.816005
299.615247	8000.123274	11.403047	-0.060900	4.816010
299.458173	8000.166365	11.408051	-0.060871	4.816024
299.591504	8000.135666	11.413056	-0.060896	4.816014
299.701796	8000.160125	11.418061	-0.060916	4.816021
299.572846	8000.117156	11.423066	-0.060892	4.816009
299.861456	8000.145938	11.428071	-0.060946	4.816016
299.856581	8000.118060	11.433075	-0.060945	4.816008
300.015888	8000.120968	11.438080	-0.060975	4.816008
299.880370	8000.173004	11.443085	-0.060949	4.816024
299.776146	8000.154000	11.448090	-0.060930	4.816019
299.943701	8000.180573	11.453095	-0.060961	4.816025
299.656875	8000.221295	11.458099	-0.060908	4.816039
299.771636	8000.189188	11.463104	-0.060929	4.816029
299.557315	8000.210927	11.468109	-0.060889	4.816036
299.423511	8000.177488	11.473114	-0.060864	4.816027
299.500755	8000.213100	11.478119	-0.060879	4.816037
299.677714	8000.217400	11.483123	-0.060912	4.816038
299.748076	8000.160968	11.488128	-0.060925	4.816021
300.038736	8000.150243	11.493133	-0.060979	4.816016
299.892309	8000.122986	11.498138	-0.060952	4.816009
299.813765	8000.162167	11.503143	-0.060937	4.816021
299.695814	8000.150394	11.508147	-0.060915	4.816018
299.756973	8000.118378	11.513152	-0.060926	4.816008
299.945998	8000.185958	11.518157	-0.060962	4.816027
299.662200	8000.170088	11.523162	-0.060909	4.816024
299.584610	8000.176153	11.528167	-0.060894	4.816026
299.540350	8000.135799	11.533171	-0.060886	4.816015
299.577064	8000.179221	11.538176	-0.060893	4.816027
299.635562	8000.196322	11.543181	-0.060904	4.816032
299.797100	8000.160793	11.548186	-0.060934	4.816020
299.774785	8000.182831	11.553191	-0.060930	4.816027
299.839495	8000.169049	11.558195	-0.060942	4.816023
299.713633	8000.157132	11.563200	-0.060918	4.816020
299.681876	8000.167240	11.568205	-0.060912	4.816023
299.699130	8000.089532	11.573210	-0.060916	4.816000
299.802982	8000.165175	11.578215	-0.060935	4.816022
299.739344	8000.159738	11.583219	-0.060923	4.816020
299.621441	8000.193925	11.588224	-0.060901	4.816031
299.751632	8000.147137	11.593229	-0.060925	4.816017
299.948123	8000.125072	11.598234	-0.060962	4.816009
299.722549	8000.173326	11.603239	-0.060920	4.816025
299.553432	8000.169169	11.608243	-0.060888	4.816024
299.538856	8000.135770	11.613248	-0.060886	4.816015
299.715517	8000.173197	11.618253	-0.060919	4.816025
299.658080	8000.199938	11.623258	-0.060908	4.816033
299.755547	8000.176066	11.628263	-0.060926	4.816025
299.445399	8000.211018	11.633267	-0.060868	4.816037
299.724787	8000.142371	11.638272	-0.060920	4.816015
299.689483	8000.148139	11.643277	-0.060914	4.816017
299.762962	8000.069319	11.648282	-0.060927	4.815994
299.700772	8000.144069	11.653287	-0.060916	4.816016
299.436842	8000.147802	11.658291	-0.060867	4.816019
299.504621	8000.200342	11.663296	-0.060879	4.816034
299.760021	8000.203936	11.668301	-0.060927	4.816033
299.431116	8000.156247	11.673306	-0.060866	4.816021
299.588641	8000.211495	11.678311	-0.060895	4.816036
299.625018	8000.149099	11.683315	-0.060902	4.816018
299.856328	8000.149046	11.688320	-0.060945	4.816017
299.912955	8000.124429	11.693325	-0.060955	4.816009
299.756716	8000.146159	11.698330	-0.060926	4.816016
299.920454	8000.185488	11.703335	-0.060957	4.816027
299.804546	8000.166271	11.708339	-0.060935	4.816022
299.854818	8000.138330	11.713344	-0.060945	4.816014
299.767772	8000.136741	11.718349	-0.060928	4.816014
299.783622	8000.100691	11.723354	-0.060931	4.816003
299.635230	8000.193106	11.728359	-0.060904	4.816031
299.757229	8000.181438	11.733363	-0.060926	4.816027
299.801671	8000.180112	11.738368	-0.060935	4.816026
299.768260	8000.228668	11.743373	-0.060928	4.816040
299.831347	8000.177447	11.748378	-0.060940	4.816025
299.954667	8000.185043	11.753383	-0.060963	4.816027
299.610077	8000.217229	11.758387	-0.060899	4.816038
299.738932	8000.110562	11.763392	-0.060923	4.816006
299.969886	8000.122260	11.768397	-0.060966	4.816008
299.770771	8000.163515	11.773402	-0.060929	4.816021
299.832783	8000.164647	11.778407	-0.060940	4.816021
299.557891	8000.178867	11.783411	-0.060889	4.816027
299.696196	8000.209181	11.788416	-0.060915	4.816035
299.721664	8000.239573	11.793421	-0.060920	4.816044
299.267670	8000.212046	11.798426	-0.060835	4.816038
299.698449	8000.198534	11.803431	-0.060915	4.816032
299.774645	8000.234127	11.808435	-0.060930	4.816042
299.925336	8000.131065	11.813440	-0.060958	4.816011
300.147403	8000.212075	11.818445	-0.060999	4.816034
299.769064	8000.185928	11.823450	-0.060929	4.816028
299.919318	8000.095684	11.828455	-0.060956	4.816001
299.972963	8000.129797	11.833459	-0.060966	4.816010
299.836820	8000.188234	11.838464	-0.060941	4.816028
299.831503	8000.219132	11.843469	-0.060940	4.816037
299.509686	8000.204706	11.848474	-0.060880	4.816035
299.671388	8000.226897	11.853479	-0.060910	4.816040
299.334979	8000.249613	11.858483	-0.060848	4.816049
299.244594	8000.228724	11.863488	-0.060831	4.816043
299.758353	8000.234897	11.868493	-0.060927	4.816042
299.911226	8000.167146	11.873498	-0.060955	4.816022
299.712458	8000.206270	11.878503	-0.060918	4.816034
299.970979	8000.186407	11.883507	-0.060966	4.816027
299.969843	8000.130808	11.888512	-0.060966	4.816011
299.996280	8000.206108	11.893517	-0.060971	4.816033
299.496116	8000.218352	11.898522	-0.060878	4.816039
299.720843	8000.167945	11.903527	-0.060920	4.816023
299.739601	8000.259137	11.908531	-0.060923	4.816049
299.667498	8000.179797	11.913536	-0.060910	4.816027
299.569321	8000.236789	11.918541	-0.060891	4.816044
299.633310	8000.212306	11.923546	-0.060903	4.816036
300.059549	8000.208331	11.928551	-0.060983	4.816033
299.973842	8000.168289	11.933555	-0.060967	4.816022
300.150398	8000.138379	11.938560	-0.061000	4.816012
300.086041	8000.181025	11.943565	-0.060988	4.816025
299.810596	8000.151413	11.948570	-0.060936	4.816018
299.725495	8000.170167	11.953575	-0.060920	4.816024
299.890322	8000.152869	11.958579	-0.060951	4.816018
299.761080	8000.155853	11.963584	-0.060927	4.816019
300.067339	8000.134724	11.968589	-0.060984	4.816011
299.914381	8000.154376	11.973594	-0.060956	4.816018
300.073991	8000.175461	11.978599	-0.060985	4.816023
299.920255	8000.177998	11.983603	-0.060957	4.816025
300.144983	8000.142554	11.988608	-0.060999	4.816013
300.222017	8000.088382	11.993613	-0.061013	4.815997
299.869321	8000.123626	11.998618	-0.060947	4.816009
299.987888	8000.104415	12.003623	-0.060969	4.816003
300.097223	8000.103204	12.008627	-0.060990	4.816002
300.148963	8000.082773	12.013632	-0.060999	4.815996
300.082350	8000.193783	12.018637	-0.060987	4.816029
299.989117	8000.163222	12.023642	-0.060969	4.816020
299.898249	8000.175457	12.028647	-0.060953	4.816024
299.932748	8000.200670	12.033651	-0.060959	4.816031
299.989629	8000.103377	12.038656	-0.060970	4.816003
300.058614	8000.193349	12.043661	-0.060982	4.816029
299.850853	8000.114738	12.048666	-0.060944	4.816007
299.906780	8000.140342	12.053671	-0.060954	4.816014
299.965963	8000.201276	12.058675	-0.060965	4.816031
300.006988	8000.135758	12.063680	-0.060973	4.816012
300.255929	8000.150992	12.068685	-0.061019	4.816015
300.249298	8000.138045	12.073690	-0.061018	4.816011
300.177599	8000.107877	12.078695	-0.061005	4.816003
300.156370	8000.119246	12.083699	-0.061001	4.816006
300.159327	8000.046621	12.088704	-0.061001	4.815985
300.153621	8000.128816	12.093709	-0.061000	4.816009
300.071803	8000.085638	12.098714	-0.060985	4.815997
300.267516	8000.173648	12.103719	-0.061021	4.816022
300.128117	8000.136900	12.108723	-0.060995	4.816012
299.982225	8000.173783	12.113728	-0.060968	4.816023
299.949750	8000.194566	12.118733	-0.060962	4.816030
299.897590	8000.113452	12.123738	-0.060952	4.816006
299.940583	8000.121719	12.128743	-0.060960	4.816008
300.072952	8000.111310	12.133747	-0.060985	4.816005
300.094027	8000.064666	12.138752	-0.060989	4.815991
300.043633	8000.167422	12.143757	-0.060980	4.816021
299.868682	8000.153539	12.148762	-0.060947	4.816018
299.986818	8000.159971	12.153767	-0.060969	4.816019
299.905670	8000.172384	12.158771	-0.060954	4.816023
299.836253	8000.088818	12.163776	-0.060941	4.815999
300.141943	8000.125394	12.168781	-0.060998	4.816008
300.065050	8000.089788	12.173786	-0.060984	4.815998
300.041590	8000.102186	12.178791	-0.060979	4.816002
299.918063	8000.081760	12.183795	-0.060956	4.815997
299.998832	8000.045826	12.188800	-0.060971	4.815986
300.055650	8000.116337	12.193805	-0.060982	4.816006
299.891956	8000.082352	12.198810	-0.060951	4.815997
300.061299	8000.181638	12.203815	-0.060983	4.816025
299.904820	8000.144578	12.208819	-0.060954	4.816015
299.953424	8000.136915	12.213824	-0.060963	4.816013
299.843680	8000.205453	12.218829	-0.060942	4.816033
300.059264	8000.027690	12.223834	-0.060982	4.815980
299.967049	7999.998218	12.228839	-0.060965	4.815972
299.959476	8000.052589	12.233843	-0.060964	4.815988
299.911163	8000.069877	12.238848	-0.060955	4.815993
300.081394	8000.125356	12.243853	-0.060987	4.816009
300.167391	8000.100206	12.248858	-0.061003	4.816001
300.209786	8000.114875	12.253863	-0.061011	4.816005
300.306120	8000.145492	12.258867	-0.061028	4.816013
300.166197	8000.093771	12.263872	-0.061002	4.815999
300.246865	8000.154029	12.268877	-0.061017	4.816016
300.261244	8000.141466	12.273882	-0.061020	4.816012
300.224989	8000.126909	12.278887	-0.061013	4.816008
300.052164	8000.164368	12.283891	-0.060981	4.816020
300.078309	8000.106061	12.288896	-0.060986	4.816003
300.113927	8000.155877	12.293901	-0.060993	4.816017
300.129758	8000.162578	12.298906	-0.060996	4.816019
300.061614	8000.149577	12.303911	-0.060983	4.816016
300.201378	8000.174574	12.308915	-0.061009	4.816022
300.167039	8000.121575	12.313920	-0.061003	4.816007
300.045993	8000.140741	12.318925	-0.060980	4.816013
300.087549	8000.110504	12.323930	-0.060988	4.816004
300.118017	8000.134574	12.328935	-0.060993	4.816011
300.207098	8000.149027	12.333939	-0.061010	4.816015
300.105932	8000.109770	12.338944	-0.060991	4.816004
300.255826	8000.174499	12.343949	-0.061019	4.816022
300.135155	8000.139162	12.348954	-0.060997	4.816012
300.025141	8000.164943	12.353959	-0.060976	4.816020
300.073670	8000.171173	12.358963	-0.060985	4.816022
299.951856	8000.117645	12.363968	-0.060962	4.816007
299.746513	8000.149167	12.368973	-0.060924	4.816017
299.852060	8000.099791	12.373978	-0.060944	4.816002
299.785032	8000.187279	12.378983	-0.060931	4.816028
299.677021	8000.224853	12.383987	-0.060911	4.816040
299.812256	8000.136472	12.388992	-0.060936	4.816013
300.080320	8000.226872	12.393997	-0.060986	4.816038
299.844993	8000.202268	12.399002	-0.060943	4.816032
299.774724	8000.242669	12.404007	-0.060930	4.816045
299.803567	8000.214337	12.409011	-0.060935	4.816036
299.676717	8000.245154	12.414016	-0.060911	4.816046
299.864978	8000.246454	12.419021	-0.060946	4.816045
299.761102	8000.202873	12.424026	-0.060927	4.816033
299.825364	8000.220079	12.429031	-0.060939	4.816038
299.758219	8000.191063	12.434035	-0.060926	4.816030
299.583762	8000.215667	12.439040	-0.060894	4.816038
299.825472	8000.238250	12.444045	-0.060939	4.816043
299.851651	8000.207732	12.449050	-0.060944	4.816034
299.944238	8000.155982	12.454055	-0.060961	4.816018
299.926482	8000.222993	12.459059	-0.060958	4.816038
299.752219	8000.192022	12.464064	-0.060925	4.816030
299.917147	8000.220685	12.469069	-0.060956	4.816037
299.864317	8000.181243	12.474074	-0.060946	4.816026
300.006974	8000.218050	12.479079	-0.060973	4.816036
299.983742	8000.225107	12.484083	-0.060968	4.816038
299.885491	8000.176285	12.489088	-0.060950	4.816025
300.017643	8000.220382	12.494093	-0.060975	4.816037
300.098165	8000.150241	12.499098	-0.060990	4.816016
299.996759	8000.201830	12.504103	-0.060971	4.816031
299.999193	8000.218976	12.509107	-0.060971	4.816036
300.143639	8000.193824	12.514112	-0.060998	4.816028
300.059515	8000.255349	12.519117	-0.060983	4.816047
299.833944	8000.220234	12.524122	-0.060941	4.816038
300.065344	8000.194532	12.529127	-0.060984	4.816029
300.131578	8000.164745	12.534131	-0.060996	4.816020
299.936736	8000.107747	12.539136	-0.060960	4.816004
300.060624	8000.154899	12.544141	-0.060983	4.816017
300.126847	8000.150764	12.549146	-0.060995	4.816016
300.104907	8000.208080	12.554151	-0.060991	4.816033
300.167567	8000.241289	12.559155	-0.061003	4.816042
300.218239	8000.233663	12.564160	-0.061012	4.816040
300.017731	8000.231071	12.569165	-0.060975	4.816040
300.067461	8000.178537	12.574170	-0.060984	4.816024
300.185501	8000.257648	12.579175	-0.061006	4.816047
300.061573	8000.239353	12.584179	-0.060983	4.816042
300.117953	8000.210455	12.589184	-0.060993	4.816033
299.807423	8000.279602	12.594189	-0.060936	4.816055
300.015642	8000.229963	12.599194	-0.060974	4.816040
299.803327	8000.247463	12.604199	-0.060935	4.816046
300.065201	8000.227661	12.609203	-0.060984	4.816039
300.031461	8000.130851	12.614208	-0.060977	4.816010
300.011418	8000.199958	12.619213	-0.060974	4.816031
299.786525	8000.173407	12.624218	-0.060932	4.816024
299.630794	8000.229348	12.629223	-0.060903	4.816041
300.175476	8000.187990	12.634227	-0.061004	4.816026
300.062319	8000.131414	12.639232	-0.060983	4.816010
299.646953	8000.242469	12.644237	-0.060906	4.816045
299.984076	8000.228317	12.649242	-0.060968	4.816039
300.090327	8000.217431	12.654247	-0.060988	4.816035
300.240607	8000.202005	12.659251	-0.061016	4.816030
300.067485	8000.151816	12.664256	-0.060984	4.816016
300.234775	8000.216862	12.669261	-0.061015	4.816035
300.136452	8000.203309	12.674266	-0.060997	4.816031
300.040892	8000.156674	12.679271	-0.060979	4.816018
300.033700	8000.176850	12.684275	-0.060978	4.816024
299.803339	8000.207915	12.689280	-0.060935	4.816034
299.926846	8000.244372	12.694285	-0.060958	4.816044
299.939294	8000.192227	12.699290	-0.060960	4.816029
299.766731	8000.177319	12.704295	-0.060928	4.816025
299.684182	8000.177950	12.709299	-0.060913	4.816026
299.585725	8000.225318	12.714304	-0.060894	4.816040
299.697676	8000.270114	12.719309	-0.060915	4.816053
299.499848	8000.257952	12.724314	-0.060878	4.816050
299.588625	8000.269192	12.729319	-0.060895	4.816053
299.987441	8000.226239	12.734323	-0.060969	4.816039
299.684309	8000.239943	12.739328	-0.060913	4.816044
299.858387	8000.274117	12.744333	-0.060945	4.816053
299.742427	8000.254899	12.749338	-0.060923	4.816048
299.649894	8000.293824	12.754343	-0.060906	4.816060
299.422968	8000.376255	12.759347	-0.060864	4.816085
299.694217	8000.252949	12.764352	-0.060915	4.816048
299.601374	8000.290800	12.769357	-0.060897	4.816059
299.595566	8000.252217	12.774362	-0.060896	4.816048
299.544776	8000.251289	12.779367	-0.060887	4.816048
299.812529	8000.235870	12.784371	-0.060937	4.816042
299.862222	8000.186543	12.789376	-0.060946	4.816028
299.940951	8000.224320	12.794381	-0.060960	4.816038
300.084806	8000.210915	12.799386	-0.060987	4.816034
299.875821	8000.204961	12.804391	-0.060948	4.816033
299.681825	8000.205694	12.809395	-0.060912	4.816034
300.136570	8000.178726	12.814400	-0.060997	4.816024
300.319432	8000.263296	12.819405	-0.061031	4.816048
300.179913	8000.223339	12.824410	-0.061005	4.816037
300.219624	8000.181311	12.829415	-0.061012	4.816024
300.448929	8000.207944	12.834419	-0.061055	4.816031
300.147691	8000.159690	12.839424	-0.060999	4.816018
300.055087	8000.129141	12.844429	-0.060982	4.816010
300.211519	8000.159786	12.849434	-0.061011	4.816018
300.201536	8000.229078	12.854439	-0.061009	4.816038
300.130447	8000.219229	12.859443	-0.060996	4.816036
300.086909	8000.167130	12.864448	-0.060988	4.816021
300.135785	8000.171229	12.869453	-0.060997	4.816022
300.128684	8000.158273	12.874458	-0.060995	4.816018
299.951839	8000.228793	12.879463	-0.060962	4.816040
300.098470	8000.230402	12.884467	-0.060990	4.816039
299.939472	8000.201846	12.889472	-0.060960	4.816032
300.351532	8000.244642	12.894477	-0.061037	4.816042
300.231844	8000.167638	12.899482	-0.061015	4.816020
300.219634	8000.191998	12.904487	-0.061012	4.816027
300.075250	8000.209669	12.909491	-0.060985	4.816033
300.131106	8000.143353	12.914496	-0.060996	4.816014
300.359486	8000.149661	12.919501	-0.061038	4.816014
300.059884	8000.165567	12.924506	-0.060983	4.816020
300.119475	8000.184825	12.929511	-0.060994	4.816026
299.973041	8000.219560	12.934515	-0.060966	4.816037
300.254663	8000.171261	12.939520	-0.061019	4.816021
300.202694	8000.177794	12.944525	-0.061009	4.816023
299.937113	8000.151568	12.949530	-0.060960	4.816017
300.119443	8000.155966	12.954535	-0.060994	4.816017
300.118576	8000.173051	12.959539	-0.060993	4.816022
300.146982	8000.157537	12.964544	-0.060999	4.816018
300.157046	8000.165202	12.969549	-0.061001	4.816020
300.276684	8000.139597	12.974554	-0.061023	4.816012
299.969413	8000.153226	12.979559	-0.060966	4.816017
300.184421	8000.184941	12.984563	-0.061006	4.816025
300.132916	8000.148729	12.989568	-0.060996	4.816015
300.172871	8000.171904	12.994573	-0.061004	4.816022
300.132338	8000.204297	12.999578	-0.060996	4.816031
300.304590	8000.161483	13.004583	-0.061028	4.816018
299.918292	8000.216421	13.009587	-0.060956	4.816036
299.882860	8000.131337	13.014592	-0.060950	4.816011
300.100263	8000.167371	13.019597	-0.060990	4.816021
300.036696	8000.194000	13.024602	-0.060978	4.816029
300.197444	8000.137081	13.029607	-0.061008	4.816011
300.269415	8000.174735	13.034611	-0.061022	4.816022
300.263035	8000.157517	13.039616	-0.061020	4.816017
300.243194	8000.176394	13.044621	-0.061017	4.816023
300.115677	8000.187960	13.049626	-0.060993	4.816027
300.332261	8000.181226	13.054631	-0.061033	4.816024
300.170846	8000.207137	13.059635	-0.061003	4.816032
300.221732	8000.101184	13.064640	-0.061013	4.816001
300.359655	8000.173176	13.069645	-0.061038	4.816021
300.236798	8000.155969	13.074650	-0.061015	4.816017
300.303215	8000.186040	13.079655	-0.061028	4.816025
300.407355	8000.156945	13.084659	-0.061047	4.816016
300.363035	8000.088800	13.089664	-0.061039	4.815996
300.511283	8000.129985	13.094669	-0.061067	4.816008
300.379047	8000.150015	13.099674	-0.061042	4.816014
300.522397	8000.131256	13.104679	-0.061069	4.816008
300.553273	8000.151059	13.109683	-0.061074	4.816014
300.481989	8000.107004	13.114688	-0.061061	4.816001
300.601495	8000.133769	13.119693	-0.061083	4.816008
300.581737	8000.121651	13.124698	-0.061080	4.816005
300.417739	8000.121863	13.129703	-0.061049	4.816006
300.479733	8000.180712	13.134707	-0.061061	4.816023
300.613195	8000.157497	13.139712	-0.061085	4.816015
300.557966	8000.159695	13.144717	-0.061075	4.816016
300.452177	8000.168451	13.149722	-0.061056	4.816019
300.580531	8000.152625	13.154727	-0.061079	4.816014
300.625287	8000.173750	13.159731	-0.061088	4.816020
300.388310	8000.156596	13.164736	-0.061044	4.816016
300.412809	8000.201934	13.169741	-0.061048	4.816029
300.550305	8000.186275	13.174746	-0.061074	4.816024
300.471241	8000.231860	13.179751	-0.061059	4.816038
300.465228	8000.177239	13.184755	-0.061058	4.816022
300.434915	8000.118969	13.189760	-0.061052	4.816005
300.124213	8000.162461	13.194765	-0.060994	4.816019
300.274220	8000.142755	13.199770	-0.061022	4.816013
300.297675	8000.134633	13.204775	-0.061027	4.816010
300.390554	8000.194045	13.209779	-0.061044	4.816027
300.091992	8000.137290	13.214784	-0.060988	4.816012
300.266777	8000.178959	13.219789	-0.061021	4.816023
300.330504	8000.184398	13.224794	-0.061033	4.816025
300.355422	8000.177371	13.229799	-0.061037	4.816022
300.376350	8000.187373	13.234803	-0.061041	4.816025
300.307087	8000.149767	13.239808	-0.061028	4.816015
300.384294	8000.203550	13.244813	-0.061043	4.816030
300.433252	8000.116800	13.249818	-0.061052	4.816004
300.465026	8000.052181	13.254823	-0.061058	4.815985
300.443131	8000.193936	13.259827	-0.061054	4.816027
300.234981	8000.174102	13.264832	-0.061015	4.816022
300.355955	8000.178449	13.269837	-0.061038	4.816023
300.547131	8000.162701	13.274842	-0.061073	4.816017
300.534266	8000.134676	13.279847	-0.061071	4.816009
300.485220	8000.174396	13.284851	-0.061062	4.816021
300.353051	8000.085407	13.289856	-0.061037	4.815995
300.410808	8000.127077	13.294861	-0.061048	4.816007
300.285687	8000.120517	13.299866	-0.061024	4.816006
300.529216	8000.147410	13.304871	-0.061070	4.816013
300.563325	8000.186510	13.309875	-0.061076	4.816024
300.409724	8000.113162	13.314880	-0.061048	4.816003
300.461924	8000.148318	13.319885	-0.061057	4.816013
300.485509	8000.155162	13.324890	-0.061062	4.816015
300.421175	8000.146505	13.329895	-0.061050	4.816013
300.448661	8000.176934	13.334899	-0.061055	4.816022
300.598117	8000.127291	13.339904	-0.061083	4.816006
300.623668	8000.141652	13.344909	-0.061087	4.816010
300.340217	8000.138613	13.349914	-0.061035	4.816011
300.004280	8000.004221	13.354919	-0.060972	4.815974
300.554366	8000.065568	13.359923	-0.061074	4.815989
300.546216	8000.030148	13.364928	-0.061073	4.815978
300.632225	8000.106536	13.369933	-0.061089	4.816000
300.394540	8000.134261	13.374938	-0.061045	4.816010
300.471930	8000.128192	13.379943	-0.061059	4.816007
300.399374	8000.163207	13.384947	-0.061046	4.816018
300.425103	8000.141231	13.389952	-0.061050	4.816011
300.610375	8000.136064	13.394957	-0.061085	4.816009
300.533859	8000.127185	13.399962	-0.061071	4.816007
300.666999	8000.098620	13.404967	-0.061095	4.815998
300.772337	8000.124058	13.409971	-0.061115	4.816005
300.735573	8000.150107	13.414976	-0.061108	4.816012
300.531435	8000.226542	13.419981	-0.061070	4.816036
300.658090	8000.209616	13.424986	-0.061094	4.816030
300.529622	8000.163447	13.429991	-0.061070	4.816017
300.387780	8000.233538	13.434995	-0.061044	4.816039
300.343033	8000.189967	13.440000	-0.061035	4.816026
300.297617	8000.240441	13.445005	-0.061027	4.816041
300.344518	8000.210302	13.450010	-0.061035	4.816032
300.344885	8000.129077	13.455015	-0.061035	4.816008
300.423364	8000.156162	13.460019	-0.061050	4.816016
300.541778	8000.105952	13.465024	-0.061072	4.816000
300.553781	8000.166025	13.470029	-0.061074	4.816018
300.565507	8000.177997	13.475034	-0.061077	4.816021
300.651920	8000.131477	13.480039	-0.061093	4.816007
300.696654	8000.196424	13.485043	-0.061101	4.816026
300.352868	8000.163425	13.490048	-0.061037	4.816018
300.544330	8000.156233	13.495053	-0.061073	4.816015
300.775767	8000.149771	13.500058	-0.061116	4.816012
300.682100	8000.123477	13.505063	-0.061098	4.816005
300.613822	8000.141469	13.510067	-0.061086	4.816010
300.427729	8000.129520	13.515072	-0.061051	4.816008
300.381362	8000.189597	13.520077	-0.061042	4.816026
300.393934	8000.184482	13.525082	-0.061045	4.816024
300.483726	8000.123061	13.530087	-0.061061	4.816006
300.647932	8000.208360	13.535091	-0.061092	4.816030
300.615531	8000.132949	13.540096	-0.061086	4.816008
300.674632	8000.135097	13.545101	-0.061097	4.816008
300.596324	8000.159319	13.550106	-0.061082	4.816016
300.538037	8000.151842	13.555111	-0.061071	4.816014
300.704915	8000.199780	13.560115	-0.061103	4.816027
300.900609	8000.136017	13.565120	-0.061139	4.816007
301.004596	8000.195634	13.570125	-0.061158	4.816024
300.972270	8000.173667	13.575130	-0.061152	4.816018
300.716072	8000.116614	13.580135	-0.061105	4.816003
300.867288	8000.185644	13.585139	-0.061133	4.816022
300.690042	8000.161030	13.590144	-0.061100	4.816016
300.772671	8000.192467	13.595149	-0.061115	4.816025
300.766221	8000.173109	13.600154	-0.061114	4.816019
300.676015	8000.123364	13.605159	-0.061097	4.816005
300.740221	8000.164084	13.610163	-0.061109	4.816016
300.790822	8000.101946	13.615168	-0.061118	4.815998
300.720707	8000.173347	13.620173	-0.061105	4.816019
300.821569	8000.182671	13.625178	-0.061124	4.816021
300.777889	8000.118811	13.630183	-0.061116	4.816003
300.926653	8000.162144	13.635187	-0.061144	4.816015
300.789466	8000.137193	13.640192	-0.061118	4.816008
300.802049	8000.136354	13.645197	-0.061121	4.816008
300.763724	8000.144204	13.650202	-0.061113	4.816010
300.713667	8000.135808	13.655207	-0.061104	4.816008
300.695683	8000.185715	13.660211	-0.061101	4.816023
300.841236	8000.128518	13.665216	-0.061128	4.816005
300.812114	8000.134399	13.670221	-0.061122	4.816007
300.733746	8000.145794	13.675226	-0.061108	4.816011
300.640644	8000.160126	13.680231	-0.061091	4.816016
300.776486	8000.182915	13.685235	-0.061116	4.816022
300.517156	8000.130081	13.690240	-0.061067	4.816008
300.416794	8000.167795	13.695245	-0.061049	4.816019
300.555768	8000.163920	13.700250	-0.061075	4.816017
300.550002	8000.158470	13.705255	-0.061074	4.816016
300.704983	8000.162370	13.710259	-0.061102	4.816016
300.672025	8000.171387	13.715264	-0.061096	4.816019
300.335672	8000.245407	13.720269	-0.061034	4.816042
300.447428	8000.211107	13.725274	-0.061055	4.816032
300.412423	8000.213674	13.730279	-0.061048	4.816033
300.418289	8000.193474	13.735283	-0.061049	4.816027
300.267629	8000.200342	13.740288	-0.061021	4.816030
300.410679	8000.207229	13.745293	-0.061048	4.816031
300.686568	8000.187685	13.750298	-0.061099	4.816024
300.629060	8000.137468	13.755303	-0.061088	4.816009
300.712965	8000.178547	13.760307	-0.061104	4.816021
300.509602	8000.153456	13.765312	-0.061066	4.816015
300.702242	8000.191177	13.770317	-0.061102	4.816025
300.432687	8000.170222	13.775322	-0.061052	4.816020
300.854151	8000.160817	13.780327	-0.061130	4.816015
300.794997	8000.199284	13.785331	-0.061119	4.816026
300.451634	8000.150259	13.790336	-0.061055	4.816014
300.635794	8000.148278	13.795341	-0.061090	4.816012
300.537158	8000.194575	13.800346	-0.061071	4.816026
300.402455	8000.193183	13.805351	-0.061046	4.816027
300.477480	8000.234100	13.810355	-0.061060	4.816038
300.512371	8000.244357	13.815360	-0.061067	4.816041
300.621905	8000.216430	13.820365	-0.061087	4.816032
300.445894	8000.183288	13.825370	-0.061054	4.816024
300.494812	8000.190594	13.830375	-0.061063	4.816025
300.749594	8000.228381	13.835379	-0.061111	4.816035
300.532631	8000.174183	13.840384	-0.061070	4.816020
300.605653	8000.188343	13.845389	-0.061084	4.816024
300.743254	8000.187649	13.850394	-0.061110	4.816023
300.470675	8000.154881	13.855399	-0.061059	4.816015
300.915657	8000.155526	13.860403	-0.061142	4.816013
300.710796	8000.168886	13.865408	-0.061104	4.816018
300.514034	8000.158879	13.870413	-0.061067	4.816016
300.479931	8000.180702	13.875418	-0.061061	4.816023
300.644885	8000.156994	13.880423	-0.061091	4.816015
300.736440	8000.228140	13.885427	-0.061108	4.816035
300.777937	8000.207521	13.890432	-0.061116	4.816029
300.790194	8000.239810	13.895437	-0.061118	4.816038
300.541278	8000.227782	13.900442	-0.061072	4.816036
300.406093	8000.222106	13.905447	-0.061047	4.816035
300.375942	8000.245070	13.910451	-0.061041	4.816042
300.405897	8000.206070	13.915456	-0.061047	4.816030
300.570851	8000.212289	13.920461	-0.061077	4.816031
300.456141	8000.187749	13.925466	-0.061056	4.816025
300.712843	8000.096241	13.930471	-0.061104	4.815997
300.543621	8000.204310	13.935475	-0.061072	4.816029
300.728417	8000.170275	13.940480	-0.061107	4.816018
300.782178	8000.193703	13.945485	-0.061117	4.816025
300.718383	8000.210708	13.950490	-0.061105	4.816030
300.683980	8000.130985	13.955495	-0.061099	4.816007
300.535154	8000.242633	13.960499	-0.061071	4.816040
300.429149	8000.223595	13.965504	-0.061051	4.816035
300.583037	8000.195409	13.970509	-0.061080	4.816026
300.636419	8000.177145	13.975514	-0.061090	4.816021
300.554597	8000.149999	13.980519	-0.061074	4.816013
300.790761	8000.200272	13.985523	-0.061118	4.816027
300.616760	8000.161822	13.990528	-0.061086	4.816016
300.420630	8000.210613	13.995533	-0.061050	4.816032
300.513757	8000.221933	14.000538	-0.061067	4.816035
300.564142	8000.154448	14.005543	-0.061076	4.816015
300.542950	8000.207503	14.010547	-0.061072	4.816030
300.499232	8000.124404	14.015552	-0.061064	4.816006
300.648772	8000.141030	14.020557	-0.061092	4.816010
300.491103	8000.167009	14.025562	-0.061063	4.816019
300.372126	8000.208658	14.030567	-0.061040	4.816031
300.757001	8000.203930	14.035571	-0.061112	4.816028
300.497771	8000.174612	14.040576	-0.061064	4.816021
300.654043	8000.138988	14.045581	-0.061093	4.816010
300.770177	8000.156072	14.050586	-0.061115	4.816014
300.711663	8000.109044	14.055591	-0.061104	4.816000
300.822173	8000.168779	14.060595	-0.061124	4.816017
300.906605	8000.119017	14.065600	-0.061140	4.816002
300.927044	8000.246582	14.070605	-0.061144	4.816040
300.889700	8000.198871	14.075610	-0.061137	4.816026
300.854717	8000.172580	14.080615	-0.061130	4.816018
300.982689	8000.183468	14.085619	-0.061154	4.816021
300.994632	8000.133450	14.090624	-0.061156	4.816006
300.720530	8000.213951	14.095629	-0.061105	4.816031
300.656421	8000.201023	14.100634	-0.061093	4.816028
300.846243	8000.145703	14.105639	-0.061129	4.816010
300.623093	8000.159798	14.110643	-0.061087	4.816016
300.513877	8000.174905	14.115648	-0.061067	4.816021
300.613915	8000.164974	14.120653	-0.061085	4.816017
300.511110	8000.212263	14.125658	-0.061066	4.816032
300.376250	8000.210869	14.130663	-0.061041	4.816032
300.576394	8000.245521	14.135667	-0.061079	4.816041
300.807502	8000.205919	14.140672	-0.061122	4.816028
300.790752	8000.194925	14.145677	-0.061118	4.816025
300.761132	8000.215760	14.150682	-0.061113	4.816031
300.682431	8000.202566	14.155687	-0.061098	4.816028
300.717981	8000.226729	14.160691	-0.061105	4.816035
300.438243	8000.188486	14.165696	-0.061053	4.816025
300.736157	8000.186445	14.170701	-0.061108	4.816023
300.700837	8000.166561	14.175706	-0.061102	4.816017
300.555327	8000.169248	14.180711	-0.061075	4.816019
300.685211	8000.262471	14.185715	-0.061099	4.816045
300.637561	8000.240224	14.190720	-0.061090	4.816039
300.756876	8000.194305	14.195725	-0.061112	4.816025
300.902595	8000.194829	14.200730	-0.061139	4.816025
301.107611	8000.214606	14.205735	-0.061177	4.816029
300.929785	8000.243423	14.210739	-0.061144	4.816039
300.710169	8000.228723	14.215744	-0.061103	4.816035
300.983595	8000.246544	14.220749	-0.061154	4.816039
300.546887	8000.235360	14.225754	-0.061073	4.816038
300.500243	8000.209925	14.230759	-0.061064	4.816031
300.666945	8000.255723	14.235763	-0.061095	4.816044
300.790362	8000.183159	14.240768	-0.061118	4.816022
300.832139	8000.187128	14.245773	-0.061126	4.816023
300.813051	8000.223120	14.250778	-0.061123	4.816033
300.771725	8000.160372	14.255783	-0.061115	4.816015
300.717723	8000.245962	14.260787	-0.061105	4.816040
300.775832	8000.194650	14.265792	-0.061116	4.816025
300.812837	7999.212019	14.270797	-0.061122	4.815738

300.755850	7996.033810	14.275802	-0.061109	4.814810
300.661141	7990.564065	14.280807	-0.061088	4.813212
300.604554	7983.903027	14.285811	-0.061073	4.811265
300.602964	7976.626635	14.290816	-0.061068	4.809137
300.563602	7969.026364	14.295821	-0.061056	4.806914
300.446688	7961.248082	14.300826	-0.061029	4.804637
300.526994	7953.379929	14.305831	-0.061039	4.802333
300.516567	7945.372314	14.310835	-0.061032	4.799986
300.256112	7937.459206	14.315840	-0.060978	4.797668
300.398682	7929.369392	14.320845	-0.060999	4.795295
300.420807	7921.447506	14.325850	-0.060998	4.792970
300.434940	7913.346468	14.330855	-0.060996	4.790592
300.261831	7905.485566	14.335859	-0.060958	4.788284
300.284237	7897.408561	14.340864	-0.060957	4.785910
300.088654	7889.411792	14.345869	-0.060915	4.783560
299.872713	7881.415541	14.350874	-0.060870	4.781209
299.516828	7873.372409	14.355879	-0.060798	4.778843
299.889367	7865.432289	14.360883	-0.060863	4.776503
299.830192	7857.354991	14.365888	-0.060846	4.774124
299.763949	7849.388604	14.370893	-0.060829	4.771776
299.860740	7841.369244	14.375898	-0.060842	4.769411
299.738183	7833.406791	14.380903	-0.060814	4.767062
299.754029	7825.347688	14.385907	-0.060811	4.764683
299.728822	7817.415699	14.390912	-0.060802	4.762341
299.732830	7809.378169	14.395917	-0.060797	4.759966
299.537690	7801.464462	14.400922	-0.060756	4.757627
299.407852	7793.374083	14.405927	-0.060726	4.755235
299.560545	7785.326318	14.410931	-0.060749	4.752853
299.516619	7777.308481	14.415936	-0.060736	4.750479
299.508777	7769.340442	14.420941	-0.060729	4.748119
299.327687	7761.304714	14.425946	-0.060690	4.745738
299.091343	7753.321895	14.430951	-0.060641	4.743372
299.384114	7745.372675	14.435955	-0.060690	4.741013
299.412767	7737.314815	14.440960	-0.060690	4.738621
299.485397	7729.364537	14.445965	-0.060699	4.736260
298.982257	7721.409509	14.450970	-0.060600	4.733898
299.127444	7713.290603	14.455975	-0.060622	4.731484
299.117802	7705.350388	14.460979	-0.060615	4.729123
298.943495	7697.337889	14.465984	-0.060577	4.726739
298.919343	7689.269255	14.470989	-0.060567	4.724337
299.027838	7681.333971	14.475994	-0.060582	4.721973
298.813030	7673.313422	14.480999	-0.060537	4.719583
298.614047	7665.405008	14.486003	-0.060495	4.717226
298.821855	7657.328880	14.491008	-0.060528	4.714816
298.743193	7649.310503	14.496013	-0.060508	4.712423
298.608720	7641.309296	14.501018	-0.060478	4.710034
298.540232	7633.280438	14.506023	-0.060460	4.707635
298.588154	7625.278694	14.511027	-0.060464	4.705243
298.532169	7617.360441	14.516032	-0.060448	4.702875
298.409638	7609.345491	14.521037	-0.060420	4.700477
298.299488	7601.378579	14.526042	-0.060395	4.698092
298.379065	7593.247498	14.531047	-0.060404	4.695657
298.148969	7585.373254	14.536051	-0.060356	4.693297
298.401169	7577.241454	14.541056	-0.060398	4.690858
298.362581	7569.322745	14.546061	-0.060385	4.688483
298.243466	7561.320116	14.551066	-0.060358	4.686081
298.194690	7553.280589	14.556071	-0.060344	4.683667
298.257524	7545.307321	14.561075	-0.060350	4.681271
298.075570	7537.323957	14.566080	-0.060311	4.678872
297.899759	7529.359338	14.571085	-0.060273	4.676476
298.014182	7521.227572	14.576090	-0.060289	4.674029
298.013232	7513.086855	14.581095	-0.060284	4.671578
297.976225	7505.203004	14.586099	-0.060272	4.669203
297.843298	7497.194203	14.591104	-0.060242	4.666789
297.958078	7489.207598	14.596109	-0.060258	4.664381
297.834203	7481.284784	14.601114	-0.060230	4.661991
297.679377	7473.237713	14.606119	-0.060196	4.659562
298.029974	7465.279173	14.611123	-0.060256	4.657157
297.891447	7457.238505	14.616128	-0.060225	4.654728
297.737617	7449.258802	14.621133	-0.060191	4.652315
297.730249	7441.200407	14.626138	-0.060184	4.649878
297.675336	7433.237821	14.631143	-0.060169	4.647468
297.469252	7425.232375	14.636147	-0.060125	4.645044
297.377821	7417.261532	14.641152	-0.060103	4.642629
297.302113	7409.207422	14.646157	-0.060084	4.640188
297.166042	7401.251017	14.651162	-0.060053	4.637775
297.004142	7393.226727	14.656167	-0.060018	4.635340
297.126176	7385.233345	14.661171	-0.060035	4.632913
296.997250	7377.211497	14.666176	-0.060006	4.630476
296.873616	7369.212431	14.671181	-0.059978	4.628045
296.878893	7361.201544	14.676186	-0.059973	4.625609
297.015459	7353.142889	14.681191	-0.059994	4.623157
296.836887	7345.226166	14.686195	-0.059955	4.620747
296.746457	7337.193938	14.691200	-0.059933	4.618301
296.540132	7329.249777	14.696205	-0.059890	4.615880
296.778520	7321.179589	14.701210	-0.059929	4.613419
296.594259	7313.114020	14.706215	-0.059889	4.610959
296.766105	7305.178047	14.711219	-0.059916	4.608536
296.876463	7297.152095	14.716224	-0.059931	4.606085
296.747046	7289.188390	14.721229	-0.059902	4.603652
296.603824	7281.216694	14.726234	-0.059870	4.601215
296.358756	7273.211480	14.731239	-0.059819	4.598766
296.031721	7265.256501	14.736243	-0.059753	4.596332
295.648314	7257.217189	14.741248	-0.059677	4.593870
296.125032	7249.123184	14.746253	-0.059760	4.591390
296.007298	7241.114997	14.751258	-0.059733	4.588935
296.042036	7233.077494	14.756263	-0.059734	4.586470
296.551592	7225.077554	14.761267	-0.059824	4.584015
296.272674	7217.140335	14.766272	-0.059767	4.581578
296.212367	7209.132039	14.771277	-0.059750	4.579118
296.277807	7201.140107	14.776282	-0.059757	4.576662
296.319347	7193.112901	14.781287	-0.059760	4.574193
296.009348	7185.148418	14.786291	-0.059697	4.571742
295.851533	7177.117089	14.791296	-0.059662	4.569270
295.973210	7169.105820	14.796301	-0.059680	4.566802
295.979886	7161.114289	14.801306	-0.059676	4.564339
295.812229	7153.147745	14.806311	-0.059639	4.561883
295.869313	7145.155639	14.811315	-0.059645	4.559417
295.657003	7137.184779	14.816320	-0.059600	4.556956
295.741859	7129.117380	14.821325	-0.059610	4.554464
295.953633	7121.135770	14.826330	-0.059645	4.551998
295.864669	7113.051428	14.831335	-0.059623	4.549498
295.587706	7105.146783	14.836339	-0.059566	4.547052
295.385141	7097.093969	14.841344	-0.059523	4.544560
295.598628	7089.146793	14.846349	-0.059558	4.542098
295.461992	7081.097544	14.851354	-0.059527	4.539604
295.329355	7073.133295	14.856359	-0.059497	4.537134
295.345268	7065.107367	14.861363	-0.059495	4.534645
295.388860	7057.077672	14.866368	-0.059498	4.532152
295.392695	7049.044543	14.871373	-0.059493	4.529658
295.670761	7041.134964	14.876378	-0.059540	4.527200
295.576647	7033.069945	14.881383	-0.059517	4.524693
295.524010	7025.190817	14.886387	-0.059502	4.522242
295.283415	7017.112500	14.891392	-0.059452	4.519727
295.114620	7009.186686	14.896397	-0.059416	4.517258
295.079991	7001.125222	14.901402	-0.059404	4.514746
294.798705	6993.040799	14.906407	-0.059346	4.512225
294.854396	6985.034853	14.911411	-0.059351	4.509728
294.812243	6977.071987	14.916416	-0.059338	4.507243
294.929847	6969.034475	14.921421	-0.059355	4.504733
294.941049	6961.112039	14.926426	-0.059352	4.502257
294.799758	6953.015381	14.931431	-0.059320	4.499726
294.762662	6945.127102	14.936435	-0.059308	4.497258
294.469138	6937.073631	14.941440	-0.059248	4.494737
294.587030	6929.028530	14.946445	-0.059265	4.492218
294.753905	6921.068189	14.951450	-0.059291	4.489724
294.392359	6913.092703	14.956455	-0.059218	4.487222
294.452767	6905.071470	14.961459	-0.059224	4.484706
294.538503	6897.059475	14.966464	-0.059235	4.482192
294.545421	6889.028797	14.971469	-0.059231	4.479670
294.487122	6881.105549	14.976474	-0.059215	4.477180
294.314075	6873.039885	14.981479	-0.059178	4.474644
294.360569	6865.034339	14.986483	-0.059181	4.472126
294.178108	6857.023605	14.991488	-0.059142	4.469604
294.247591	6849.036792	14.996493	-0.059150	4.467089
294.268137	6841.042074	15.001498	-0.059148	4.464569
294.011360	6833.058670	15.006503	-0.059095	4.462052
293.878085	6825.037039	15.011507	-0.059065	4.459521
294.141937	6817.011844	15.016512	-0.059109	4.456988
293.970287	6809.056114	15.021517	-0.059072	4.454475
293.644290	6801.051342	15.026522	-0.059006	4.451944
293.742519	6792.980362	15.031527	-0.059019	4.449393
293.951294	6785.054781	15.036531	-0.059053	4.446886
293.599233	6777.026719	15.041536	-0.058982	4.444344
293.463345	6769.085592	15.046541	-0.058952	4.441828
293.269297	6761.076846	15.051546	-0.058910	4.439289
293.365187	6753.022968	15.056551	-0.058923	4.436736
293.472809	6745.022737	15.061555	-0.058938	4.434198
293.354116	6736.944368	15.066560	-0.058910	4.431633
293.159376	6728.983718	15.071565	-0.058869	4.429103
293.219174	6720.987079	15.076570	-0.058875	4.426562
293.094026	6712.978807	15.081575	-0.058846	4.424015
293.225285	6704.984528	15.086579	-0.058865	4.421471
293.053454	6696.975390	15.091584	-0.058828	4.418921
292.962544	6688.998251	15.096589	-0.058806	4.416379
293.013210	6681.020835	15.101594	-0.058810	4.413837
292.938647	6672.908857	15.106599	-0.058791	4.411249
293.017575	6664.993125	15.111603	-0.058801	4.408723
292.892988	6656.966591	15.116608	-0.058772	4.406160
292.934356	6648.996070	15.121613	-0.058775	4.403614
292.739220	6641.028801	15.126618	-0.058733	4.401066
292.722724	6633.010838	15.131623	-0.058725	4.398501
292.602704	6625.064490	15.136627	-0.058697	4.395957
292.509089	6617.014205	15.141632	-0.058675	4.393379
292.371962	6608.925545	15.146637	-0.058644	4.390786
292.341566	6601.001621	15.151642	-0.058633	4.388246
292.253408	6592.956761	15.156647	-0.058611	4.385664
292.237542	6585.028291	15.161651	-0.058603	4.383119
292.361114	6576.984557	15.166656	-0.058621	4.380536
292.286764	6569.013900	15.171661	-0.058602	4.377974
292.184300	6561.014449	15.176666	-0.058578	4.375402
292.096134	6552.986527	15.181671	-0.058556	4.372818
292.375932	6544.933767	15.186675	-0.058603	4.370227
292.036270	6536.948825	15.191680	-0.058535	4.367653
291.780307	6528.979844	15.196685	-0.058482	4.365083
292.198917	6521.013291	15.201690	-0.058554	4.362516
291.962280	6512.964451	15.206695	-0.058505	4.359917
292.266999	6505.029520	15.211699	-0.058557	4.357357
292.129424	6496.956601	15.216704	-0.058526	4.354748
291.978085	6488.841534	15.221709	-0.058492	4.352124
292.086495	6480.855827	15.226714	-0.058507	4.349541
291.869422	6472.935988	15.231719	-0.058462	4.346976
291.801769	6464.945766	15.236723	-0.058444	4.344388
291.694081	6457.031428	15.241728	-0.058419	4.341823
291.606819	6448.925055	15.246733	-0.058397	4.339194
291.843446	6440.975945	15.251738	-0.058436	4.336616
291.538742	6432.943284	15.256743	-0.058374	4.334007
291.649762	6424.967721	15.261747	-0.058390	4.331417
291.455187	6416.959918	15.266752	-0.058348	4.328813
291.471184	6408.932529	15.271757	-0.058346	4.326202
291.596474	6400.951831	15.276762	-0.058364	4.323606
291.161059	6392.951233	15.281767	-0.058278	4.320998
290.927711	6385.085475	15.286771	-0.058229	4.318433
290.672464	6377.001900	15.291776	-0.058176	4.315796
290.996961	6368.940524	15.296781	-0.058231	4.313169
291.134574	6360.927210	15.301786	-0.058252	4.310554
291.043307	6352.872139	15.306791	-0.058230	4.307922
291.347957	6344.844772	15.311795	-0.058281	4.305301
291.142556	6336.950980	15.316800	-0.058238	4.302718
291.256039	6328.915563	15.321805	-0.058254	4.300090
291.264982	6320.987492	15.326810	-0.058250	4.297494
291.001779	6312.878972	15.331815	-0.058196	4.294836
290.880884	6304.913202	15.336819	-0.058168	4.292224
290.940642	6296.912917	15.341824	-0.058174	4.289600
290.814236	6288.904774	15.346829	-0.058145	4.286971
290.843180	6280.928328	15.351834	-0.058145	4.284351
290.522111	6272.960382	15.356839	-0.058081	4.281730
290.386948	6264.976832	15.361843	-0.058050	4.279104
290.252884	6256.985888	15.366848	-0.058020	4.276474
290.329941	6248.908482	15.371853	-0.058029	4.273815
290.535301	6240.918174	15.376858	-0.058062	4.271184
290.524073	6232.854787	15.381863	-0.058055	4.268526
290.500556	6224.874334	15.386867	-0.058045	4.265894
290.578638	6216.900983	15.391872	-0.058054	4.263263
290.334536	6208.903885	15.396877	-0.058004	4.260620
290.416612	6200.942202	15.401882	-0.058014	4.257990
290.189664	6192.932058	15.406887	-0.057966	4.255339
289.848798	6184.983743	15.411891	-0.057898	4.252706
289.890896	6176.879606	15.416896	-0.057900	4.250024
290.001963	6168.853176	15.421901	-0.057916	4.247365
290.001286	6160.881788	15.426906	-0.057910	4.244723
289.726038	6152.966028	15.431911	-0.057854	4.242095
290.099632	6144.881647	15.436915	-0.057918	4.239415
290.107984	6136.957844	15.441920	-0.057915	4.236783
289.901368	6128.894603	15.446925	-0.057871	4.234102
289.769933	6120.953681	15.451930	-0.057841	4.231460
289.927107	6112.860610	15.456935	-0.057865	4.228769
289.666449	6104.915578	15.461939	-0.057812	4.226121
289.725655	6096.916026	15.466944	-0.057817	4.223456
289.594739	6088.931589	15.471949	-0.057788	4.220793
289.612976	6080.982602	15.476954	-0.057786	4.218142
289.378734	6072.945842	15.481959	-0.057737	4.215457
289.017356	6065.012367	15.486963	-0.057665	4.212803
289.205158	6056.873781	15.491968	-0.057694	4.210085
289.499584	6048.885626	15.496973	-0.057744	4.207416
289.361827	6040.917079	15.501978	-0.057713	4.204748
289.291454	6032.955376	15.506983	-0.057695	4.202081
289.297521	6024.965735	15.511987	-0.057691	4.199404
289.051800	6016.952489	15.516992	-0.057640	4.196715
289.014695	6008.894433	15.521997	-0.057628	4.194011
289.165490	6000.827487	15.527002	-0.057651	4.191304
288.630586	5992.898273	15.532007	-0.057546	4.188635
288.915172	5984.892338	15.537011	-0.057594	4.185947
288.626865	5976.942685	15.542016	-0.057535	4.183269
288.721582	5968.879610	15.547021	-0.057547	4.180556
288.851901	5960.891965	15.552026	-0.057566	4.177867
288.768499	5952.857860	15.557031	-0.057545	4.175159
288.814926	5944.923885	15.562035	-0.057549	4.172484
288.483812	5936.884115	15.567040	-0.057482	4.169767
288.792878	5928.890034	15.572045	-0.057534	4.167071
288.948886	5920.868117	15.577050	-0.057558	4.164362
288.692477	5912.944234	15.582055	-0.057505	4.161680
288.499786	5904.981967	15.587059	-0.057464	4.158983
288.281219	5896.950217	15.592064	-0.057418	4.156262
288.535648	5888.885046	15.597069	-0.057460	4.153532
288.587667	5880.842906	15.602074	-0.057465	4.150806
288.449933	5872.860268	15.607079	-0.057434	4.148097
288.415645	5864.850904	15.612083	-0.057422	4.145377
288.243416	5856.888270	15.617088	-0.057385	4.142671
288.183000	5848.881177	15.622093	-0.057369	4.139948
288.191173	5840.941249	15.627098	-0.057365	4.137248
288.111848	5832.894922	15.632103	-0.057345	4.134508
288.085780	5824.917173	15.637107	-0.057335	4.131791
288.231486	5816.874565	15.642112	-0.057357	4.129052
288.143206	5808.841831	15.647117	-0.057335	4.126311
288.084602	5800.915853	15.652122	-0.057319	4.123605
288.027671	5792.886291	15.657127	-0.057303	4.120863
287.953588	5784.936700	15.662131	-0.057284	4.118145
287.696921	5776.899487	15.667136	-0.057231	4.115394
287.614104	5768.877882	15.672141	-0.057210	4.112648
287.851163	5760.872813	15.677146	-0.057249	4.109910
287.787568	5752.838453	15.682151	-0.057232	4.107157
287.769586	5744.826041	15.687155	-0.057224	4.104409
287.839875	5736.848490	15.692160	-0.057232	4.101673
287.658927	5728.899224	15.697165	-0.057193	4.098942
287.415667	5720.931325	15.702170	-0.057142	4.096201
287.436105	5712.892681	15.707175	-0.057141	4.093438
287.677287	5704.914627	15.712179	-0.057181	4.090696
287.590699	5696.922547	15.717184	-0.057159	4.087944
287.398582	5688.893718	15.722189	-0.057118	4.085176
287.437931	5680.968370	15.727194	-0.057120	4.082444
287.209212	5672.932894	15.732199	-0.057073	4.079670
287.060493	5664.974931	15.737203	-0.057040	4.076921
287.126154	5656.927313	15.742208	-0.057047	4.074142
287.111341	5648.892831	15.747213	-0.057039	4.071364
286.984549	5640.935022	15.752218	-0.057010	4.068610
287.063378	5632.897887	15.757223	-0.057019	4.065829
287.075586	5624.949969	15.762227	-0.057016	4.063077
286.851902	5616.920512	15.767232	-0.056970	4.060291
286.857537	5608.949551	15.772237	-0.056965	4.057526
286.737376	5600.945940	15.777242	-0.056938	4.054747
286.708127	5592.941494	15.782247	-0.056927	4.051966
286.617977	5584.911817	15.787251	-0.056905	4.049174
286.589563	5576.915707	15.792256	-0.056895	4.046393
286.481115	5568.926611	15.797261	-0.056869	4.043611
286.640870	5560.957079	15.802266	-0.056894	4.040837
286.506179	5552.988164	15.807271	-0.056863	4.038058
286.455906	5544.942530	15.812275	-0.056849	4.035252
286.527178	5536.856295	15.817280	-0.056857	4.032431
286.350592	5528.820980	15.822285	-0.056819	4.029622
286.323113	5520.879702	15.827290	-0.056808	4.026846
286.264605	5512.873845	15.832295	-0.056792	4.024045
286.194062	5504.916021	15.837299	-0.056774	4.021259
286.177959	5496.935572	15.842304	-0.056766	4.018464
286.143190	5488.906281	15.847309	-0.056754	4.015649
286.258513	5480.921533	15.852314	-0.056770	4.012851
286.091750	5472.871870	15.857319	-0.056734	4.010023
286.280413	5464.943967	15.862323	-0.056764	4.007242
286.273120	5456.879124	15.867328	-0.056757	4.004407
285.928405	5448.952884	15.872333	-0.056688	4.001614
286.103134	5440.933978	15.877338	-0.056715	3.998795
285.701879	5432.963974	15.882343	-0.056635	3.995982
285.873444	5424.906014	15.887347	-0.056662	3.993144
285.710363	5416.897030	15.892352	-0.056627	3.990317
285.678597	5408.893194	15.897357	-0.056615	3.987492
285.729732	5400.908975	15.902362	-0.056620	3.984673
285.616188	5392.953763	15.907367	-0.056593	3.981859
285.725389	5384.921718	15.912371	-0.056609	3.979020
285.576818	5376.951259	15.917376	-0.056576	3.976196
285.251630	5368.969983	15.922381	-0.056510	3.973364
285.230868	5360.958470	15.927386	-0.056501	3.970524
285.350340	5352.940922	15.932391	-0.056518	3.967682
285.244988	5344.958011	15.937395	-0.056493	3.964847
284.994457	5337.016645	15.942400	-0.056441	3.962022
285.030646	5328.961359	15.947405	-0.056443	3.959159
285.323423	5320.995416	15.952410	-0.056492	3.956330
285.193440	5312.946366	15.957415	-0.056463	3.953462
285.160814	5304.948523	15.962419	-0.056451	3.950613
284.886253	5296.986408	15.967424	-0.056395	3.947769
284.875647	5288.947516	15.972429	-0.056388	3.944901
284.616524	5280.998125	15.977434	-0.056334	3.942059
284.816192	5272.942438	15.982439	-0.056366	3.939184
284.791868	5264.968016	15.987443	-0.056357	3.936332
284.393746	5256.986205	15.992448	-0.056277	3.933469
284.771919	5248.918364	15.997453	-0.056342	3.930587
284.586092	5240.971084	16.002458	-0.056303	3.927736
284.497167	5232.965701	16.007463	-0.056281	3.924864
284.432526	5225.035464	16.012467	-0.056264	3.922017
284.514570	5217.015087	16.017472	-0.056274	3.919138
284.381585	5209.015647	16.022477	-0.056244	3.916261
284.245876	5200.985840	16.027482	-0.056213	3.913370
284.181219	5192.940249	16.032487	-0.056196	3.910474
284.078783	5184.992674	16.037491	-0.056172	3.907609
283.956849	5176.979236	16.042496	-0.056144	3.904718
283.806619	5169.056288	16.047501	-0.056111	3.901858
284.082628	5161.000740	16.052506	-0.056157	3.898955
283.878299	5153.010261	16.057511	-0.056113	3.896065
284.032707	5144.981447	16.062515	-0.056137	3.893165
283.965494	5136.955340	16.067520	-0.056119	3.890260
283.973664	5128.948594	16.072525	-0.056116	3.887361
283.875561	5121.012786	16.077530	-0.056092	3.884484
283.637833	5113.043724	16.082535	-0.056043	3.881590
283.758906	5105.018039	16.087539	-0.056060	3.878680
283.671184	5096.998149	16.092544	-0.056038	3.875766
283.681305	5088.800551	16.097549	-0.056035	3.872787
283.819737	5080.815261	16.102554	-0.056055	3.869885
283.624498	5072.869956	16.107559	-0.056014	3.866989
283.501472	5064.943971	16.112563	-0.055986	3.864100
283.454841	5056.980497	16.117568	-0.055972	3.861196
283.387732	5048.977089	16.122573	-0.055954	3.858275
283.384498	5040.995135	16.127578	-0.055948	3.855361
283.246376	5032.973575	16.132583	-0.055918	3.852428
283.382362	5024.953525	16.137587	-0.055938	3.849498
283.424700	5016.967668	16.142592	-0.055940	3.846577
283.288283	5009.005328	16.147597	-0.055910	3.843658
283.394541	5001.035761	16.152602	-0.055924	3.840740
283.118630	4993.055003	16.157607	-0.055868	3.837807
282.996588	4985.027738	16.162611	-0.055840	3.834859
283.028264	4977.011761	16.167616	-0.055840	3.831915
282.901885	4969.026030	16.172621	-0.055812	3.828977
282.970203	4961.020327	16.177626	-0.055819	3.826033
282.931324	4953.027629	16.182631	-0.055807	3.823090
282.816120	4945.067432	16.187635	-0.055780	3.820154
282.603757	4937.104514	16.192640	-0.055735	3.817214
282.587383	4929.074131	16.197645	-0.055727	3.814250
282.598882	4921.059403	16.202650	-0.055724	3.811290
282.455111	4913.080036	16.207655	-0.055692	3.808338
282.635496	4905.054597	16.212659	-0.055720	3.805373
282.665310	4897.121563	16.217664	-0.055721	3.802438
282.599432	4889.080548	16.222669	-0.055703	3.799457
282.423150	4881.160856	16.227674	-0.055665	3.796517
282.181836	4873.063596	16.232679	-0.055615	3.793508
282.269305	4865.050358	16.237683	-0.055626	3.790534
282.297004	4857.062827	16.242688	-0.055626	3.787566
281.893547	4849.070772	16.247693	-0.055546	3.784585
282.082442	4841.098950	16.252698	-0.055576	3.781622
281.871028	4833.096627	16.257703	-0.055531	3.778636
281.796819	4825.070831	16.262707	-0.055512	3.775643
281.911559	4817.095410	16.267712	-0.055528	3.772670
281.944407	4809.044196	16.272717	-0.055529	3.769664
281.776337	4801.135853	16.277722	-0.055493	3.766705
281.635720	4793.101146	16.282727	-0.055461	3.763697
281.914772	4785.119355	16.287731	-0.055508	3.760716
281.775000	4777.164923	16.292736	-0.055477	3.757733
281.640803	4769.099994	16.297741	-0.055447	3.754707
281.557094	4761.115917	16.302746	-0.055426	3.751709
281.423891	4753.103884	16.307751	-0.055396	3.748698
281.483368	4745.071611	16.312755	-0.055402	3.745680
281.497726	4737.138177	16.317760	-0.055399	3.742697
281.559380	4729.068035	16.322765	-0.055405	3.739661
281.320819	4721.172099	16.327770	-0.055356	3.736681
281.337263	4713.114453	16.332775	-0.055354	3.733644
281.399392	4705.087815	16.337779	-0.055360	3.730617
281.284489	4697.124170	16.342784	-0.055333	3.727607
280.978479	4689.135209	16.347789	-0.055271	3.724580
281.198032	4681.199096	16.352794	-0.055307	3.721584
280.960898	4673.187573	16.357799	-0.055257	3.718545
281.095756	4665.197926	16.362803	-0.055277	3.715522
280.998785	4657.118305	16.367808	-0.055254	3.712456
280.798117	4649.092297	16.372813	-0.055211	3.709405
280.936631	4641.135996	16.377818	-0.055232	3.706387
280.657756	4633.156162	16.382823	-0.055175	3.703347
280.687032	4625.167345	16.387827	-0.055175	3.700309
280.574005	4617.213912	16.392832	-0.055149	3.697278
280.430328	4609.192867	16.397837	-0.055117	3.694218
280.447090	4601.171426	16.402842	-0.055115	3.691159
280.490817	4593.170416	16.407847	-0.055118	3.688107
280.534321	4585.180935	16.412851	-0.055121	3.685056
280.506286	4577.233748	16.417856	-0.055110	3.682017
280.519934	4569.203956	16.422861	-0.055108	3.678945
280.541950	4561.230846	16.427866	-0.055106	3.675892
280.009402	4553.242277	16.432871	-0.055002	3.672817
280.184595	4545.210609	16.437875	-0.055029	3.669741
280.368889	4537.220766	16.442880	-0.055059	3.666678
280.228968	4529.211973	16.447885	-0.055027	3.663597
280.391564	4521.223896	16.452890	-0.055052	3.660529
280.070661	4513.260999	16.457895	-0.054987	3.657456
279.849116	4505.248861	16.462899	-0.054941	3.654364
279.840102	4497.264120	16.467904	-0.054934	3.651286
279.874956	4489.216036	16.472909	-0.054935	3.648181
280.109026	4481.263941	16.477914	-0.054974	3.645116
279.859022	4473.284267	16.482919	-0.054922	3.642026
279.705426	4465.304924	16.487923	-0.054888	3.638935
279.708111	4457.323383	16.492928	-0.054883	3.635845
279.364216	4449.290208	16.497933	-0.054814	3.632723
279.557697	4441.220780	16.502938	-0.054845	3.629598
279.456133	4433.248470	16.507943	-0.054821	3.626501
279.472126	4425.282137	16.512947	-0.054819	3.623406
279.342884	4417.268457	16.517952	-0.054789	3.620287
279.463676	4409.285288	16.522957	-0.054807	3.617183
279.426451	4401.291880	16.527962	-0.054795	3.614069
279.140819	4393.289105	16.532967	-0.054736	3.610941
279.169281	4385.308201	16.537971	-0.054736	3.607828
279.301074	4377.288570	16.542976	-0.054756	3.604700
279.275684	4369.349187	16.547981	-0.054746	3.601596
279.283880	4361.364836	16.552986	-0.054742	3.598472
279.215635	4353.348993	16.557991	-0.054724	3.595332
279.055811	4345.375358	16.562995	-0.054689	3.592203
278.885624	4337.368115	16.568000	-0.054652	3.589057
278.954025	4329.346177	16.573005	-0.054660	3.585910
279.101598	4321.376422	16.578010	-0.054682	3.582783
278.854355	4313.371270	16.583015	-0.054631	3.579628
278.665057	4305.427794	16.588019	-0.054590	3.576496
278.745648	4297.410903	16.593024	-0.054600	3.573340
278.627180	4289.365604	16.598029	-0.054573	3.570164
278.651209	4281.416027	16.603034	-0.054572	3.567027
278.458754	4273.401490	16.608039	-0.054531	3.563856
278.521115	4265.413484	16.613043	-0.054537	3.560700
278.380397	4257.474989	16.618048	-0.054506	3.557554
278.444051	4249.409627	16.623053	-0.054513	3.554362
278.260574	4241.337381	16.628058	-0.054473	3.551156
278.044908	4233.404654	16.633063	-0.054428	3.548002
278.045997	4225.370344	16.638067	-0.054423	3.544812
278.310080	4217.406218	16.643072	-0.054467	3.541654
277.983043	4209.406715	16.648077	-0.054401	3.538462
277.868267	4201.444228	16.653082	-0.054374	3.535287
277.999887	4193.429052	16.658087	-0.054393	3.532097
278.024031	4185.439280	16.663091	-0.054393	3.528910
277.867813	4177.438218	16.668096	-0.054358	3.525711
277.779722	4169.471380	16.673101	-0.054337	3.522524
277.735572	4161.510043	16.678106	-0.054323	3.519338
277.728754	4153.489205	16.683111	-0.054317	3.516126
277.721732	4145.488956	16.688115	-0.054310	3.512920
277.785329	4137.440083	16.693120	-0.054317	3.509694
277.619373	4129.444069	16.698125	-0.054281	3.506478
277.722724	4121.489245	16.703130	-0.054295	3.503285
277.694964	4113.485734	16.708135	-0.054285	3.500065
277.672415	4105.535713	16.713139	-0.054275	3.496863
277.403486	4097.566274	16.718144	-0.054220	3.493644
277.289871	4089.526555	16.723149	-0.054193	3.490397
277.380409	4081.541952	16.728154	-0.054205	3.487177
277.302556	4073.569264	16.733159	-0.054185	3.483953
277.240533	4065.579619	16.738163	-0.054169	3.480719
277.320099	4057.616450	16.743168	-0.054178	3.477498
277.106667	4049.591897	16.748173	-0.054133	3.474240
277.048359	4041.558970	16.753178	-0.054117	3.470980
276.829437	4033.598512	16.758183	-0.054071	3.467741
276.756179	4025.570384	16.763187	-0.054052	3.464476
276.852187	4017.602475	16.768192	-0.054065	3.461238
276.859028	4009.593855	16.773197	-0.054061	3.457978
276.948986	4001.603040	16.778202	-0.054073	3.454724
276.801071	3993.624869	16.783207	-0.054040	3.451465
276.578740	3985.620500	16.788211	-0.053993	3.448190
276.661435	3977.623892	16.793216	-0.054004	3.444925
276.602683	3969.627861	16.798221	-0.053987	3.441652
276.533181	3961.686820	16.803226	-0.053969	3.438398
276.416992	3953.686284	16.808231	-0.053942	3.435116
276.497285	3945.634997	16.813235	-0.053952	3.431815
276.382055	3937.674878	16.818240	-0.053925	3.428543
276.214402	3929.640121	16.823245	-0.053889	3.425235
276.311405	3921.702427	16.828250	-0.053902	3.421972
276.433375	3913.667174	16.833255	-0.053919	3.418667
276.207398	3905.716515	16.838259	-0.053872	3.415382
276.051961	3897.746663	16.843264	-0.053838	3.412089
275.965377	3889.701112	16.848269	-0.053817	3.408763
276.042753	3881.749601	16.853274	-0.053826	3.405478
275.863296	3873.786194	16.858279	-0.053787	3.402177
275.894246	3865.790610	16.863283	-0.053788	3.398866
275.714258	3857.836845	16.868288	-0.053749	3.395562
275.648037	3849.669438	16.873293	-0.053731	3.392170
275.814316	3841.684662	16.878298	-0.053757	3.388858
275.665868	3833.701618	16.883303	-0.053724	3.385533
275.690837	3825.753214	16.888307	-0.053724	3.382225
275.658413	3817.809902	16.893312	-0.053713	3.378914
275.402776	3809.807864	16.898317	-0.053660	3.375568
275.750015	3801.790757	16.903322	-0.053719	3.372233
275.447879	3793.802648	16.908327	-0.053658	3.368884
275.568160	3785.815975	16.913331	-0.053675	3.365547
275.356757	3777.870520	16.918336	-0.053630	3.362213
275.176165	3769.872365	16.923341	-0.053592	3.358854
275.262894	3761.890758	16.928346	-0.053602	3.355508
275.130466	3753.851840	16.933351	-0.053573	3.352127
275.108421	3745.839854	16.938355	-0.053563	3.348757
275.173816	3737.868483	16.943360	-0.053570	3.345405
275.023601	3729.881397	16.948365	-0.053537	3.342035
274.987493	3721.897788	16.953370	-0.053525	3.338667
275.013617	3713.896183	16.958375	-0.053525	3.335290
274.934672	3705.891094	16.963379	-0.053505	3.331905
274.973997	3697.897937	16.968384	-0.053507	3.328525
274.805856	3689.897763	16.973389	-0.053470	3.325131
274.935986	3681.963770	16.978394	-0.053490	3.321773
274.961827	3673.960805	16.983399	-0.053489	3.318379
274.780997	3665.985584	16.988403	-0.053450	3.314985
274.712345	3657.958870	16.993408	-0.053432	3.311570
274.782685	3649.914320	16.998413	-0.053440	3.308149
274.804977	3641.967259	17.003418	-0.053439	3.304764
274.588343	3633.996756	17.008423	-0.053394	3.301356
274.427500	3626.059620	17.013427	-0.053358	3.297962
274.507237	3618.047329	17.018432	-0.053368	3.294541
274.189988	3610.021002	17.023437	-0.053304	3.291095
273.998986	3602.092539	17.028442	-0.053263	3.287692
273.950300	3594.065048	17.033447	-0.053249	3.284249
274.185640	3586.072208	17.038451	-0.053287	3.280828
274.174401	3578.101722	17.043456	-0.053280	3.277403
274.115898	3570.094484	17.048461	-0.053264	3.273958
274.032991	3562.098632	17.053466	-0.053243	3.270512
273.914799	3554.094162	17.058471	-0.053216	3.267058
273.798994	3546.111023	17.063475	-0.053189	3.263610
273.866368	3538.120495	17.068480	-0.053197	3.260161
273.784696	3530.146161	17.073485	-0.053176	3.256711
273.800497	3522.167121	17.078490	-0.053174	3.253258
273.778778	3514.122189	17.083495	-0.053165	3.249772
273.643251	3506.167536	17.088499	-0.053134	3.246316
273.640651	3498.184087	17.093504	-0.053129	3.242850
273.483338	3490.188928	17.098509	-0.053094	3.239368
273.541887	3482.257160	17.103514	-0.053100	3.235920
273.344962	3474.209815	17.108519	-0.053058	3.232406
273.236010	3466.177501	17.113523	-0.053032	3.228899
273.333678	3458.177006	17.118528	-0.053045	3.225411
273.429263	3450.180318	17.123533	-0.053058	3.221920
273.233716	3442.255706	17.128538	-0.053016	3.218445
273.123001	3434.255610	17.133543	-0.052990	3.214937
273.131740	3426.251013	17.138547	-0.052987	3.211428
273.080492	3418.304145	17.143552	-0.052972	3.207938
273.051789	3410.270811	17.148557	-0.052962	3.204407
272.878327	3402.353589	17.153562	-0.052924	3.200917
272.490972	3394.409255	17.158567	-0.052847	3.197403
272.716647	3386.340973	17.163571	-0.052884	3.193855
272.751649	3378.317960	17.168576	-0.052885	3.190316
272.497263	3370.347503	17.173581	-0.052832	3.186784
272.523537	3362.370648	17.178586	-0.052832	3.183256
272.683101	3354.358233	17.183591	-0.052857	3.179715
272.679291	3346.420924	17.188595	-0.052851	3.176196
272.340058	3338.447826	17.193600	-0.052782	3.172643
272.375398	3330.380553	17.198605	-0.052784	3.169061
272.429472	3322.425113	17.203610	-0.052788	3.165524
272.495467	3314.431848	17.208615	-0.052796	3.161968
272.347359	3306.486366	17.213619	-0.052763	3.158419
272.307122	3298.515010	17.218624	-0.052750	3.154860
272.087600	3290.471547	17.223629	-0.052704	3.151256
272.046880	3282.518423	17.228634	-0.052691	3.147697
271.728027	3274.560913	17.233639	-0.052627	3.144120
272.004170	3266.504625	17.238643	-0.052673	3.140520
272.096565	3258.513586	17.243648	-0.052685	3.136937
271.816543	3250.554820	17.248653	-0.052627	3.133348
271.897095	3242.549216	17.253658	-0.052637	3.129750
271.844597	3234.585227	17.258663	-0.052622	3.126161
271.580906	3226.593735	17.263667	-0.052568	3.122545
271.505494	3218.649769	17.268672	-0.052549	3.118956
271.492367	3210.627384	17.273677	-0.052541	3.115329
271.476165	3202.660164	17.278682	-0.052533	3.111723
271.397751	3194.653252	17.283687	-0.052513	3.108092
271.585836	3186.613469	17.288691	-0.052543	3.104454
271.412966	3178.684187	17.293696	-0.052505	3.100846
271.106639	3170.710948	17.298701	-0.052443	3.097207
271.239854	3162.726666	17.303706	-0.052463	3.093579
270.970967	3154.715219	17.308711	-0.052408	3.089916
270.710208	3146.746790	17.313715	-0.052354	3.086269
270.959524	3138.750361	17.318720	-0.052395	3.082627
270.882864	3130.773536	17.323725	-0.052376	3.078976
270.712369	3122.839524	17.328730	-0.052339	3.075335
270.645859	3114.739781	17.333735	-0.052321	3.071619
270.760066	3106.699569	17.338739	-0.052337	3.067934
270.885345	3098.729628	17.343744	-0.052355	3.064278
270.365934	3090.812247	17.348749	-0.052253	3.060611
270.570539	3082.835675	17.353754	-0.052286	3.056946
270.602524	3074.821219	17.358759	-0.052287	3.053252
270.328220	3066.860581	17.363763	-0.052231	3.049563
270.317871	3058.890122	17.368768	-0.052224	3.045878
270.218310	3050.899369	17.373773	-0.052200	3.042175
270.108870	3042.954425	17.378778	-0.052174	3.038488
270.232339	3034.940065	17.383783	-0.052192	3.034775
270.388816	3026.889063	17.388787	-0.052216	3.031042
270.477693	3018.922635	17.393792	-0.052227	3.027341
270.113449	3010.992047	17.398797	-0.052154	3.023630
270.135563	3003.005883	17.403802	-0.052153	3.019908
269.938589	2995.032274	17.408807	-0.052111	3.016176
269.975267	2987.016945	17.413811	-0.052113	3.012431
269.904383	2979.044119	17.418816	-0.052094	3.008696
270.007443	2971.015114	17.423821	-0.052108	3.004938
269.692578	2963.138273	17.428826	-0.052045	3.001227
269.541998	2955.165774	17.433831	-0.052011	2.997475
269.809817	2947.114928	17.438835	-0.052056	2.993701
269.627284	2939.109583	17.443840	-0.052017	2.989922
269.509514	2931.126814	17.448845	-0.051990	2.986152
269.578390	2923.163542	17.453850	-0.051997	2.982395
269.328947	2915.195789	17.458855	-0.051946	2.978616
269.174183	2907.228238	17.463859	-0.051912	2.974837
269.316616	2899.207718	17.468864	-0.051933	2.971043
269.000862	2891.270470	17.473869	-0.051869	2.967260
268.844883	2883.291014	17.478874	-0.051835	2.963461
268.827074	2875.296620	17.483879	-0.051826	2.959656
268.945734	2867.309044	17.488883	-0.051843	2.955857
269.063821	2859.260442	17.493888	-0.051860	2.952024
268.867035	2851.263244	17.498893	-0.051818	2.948194
269.046690	2843.288873	17.503898	-0.051846	2.944390
269.208142	2835.313647	17.508903	-0.051871	2.940579
268.901899	2827.398538	17.513907	-0.051809	2.936768
269.040649	2819.389832	17.518912	-0.051830	2.932930
268.709340	2811.413283	17.523917	-0.051763	2.929078
268.651321	2803.447542	17.528922	-0.051747	2.925241
268.779997	2795.449969	17.533927	-0.051765	2.921392
268.318450	2787.520078	17.538931	-0.051674	2.917541
268.563056	2779.454736	17.543936	-0.051715	2.913656
268.222203	2771.435687	17.548941	-0.051646	2.909757
268.224070	2763.500757	17.553946	-0.051641	2.905912
268.430637	2755.479920	17.558951	-0.051674	2.902031
268.113367	2747.549132	17.563955	-0.051610	2.898161
268.093053	2739.589345	17.568960	-0.051601	2.894287
268.132614	2731.528596	17.573965	-0.051603	2.890362
268.237802	2723.580240	17.578970	-0.051618	2.886490
267.897894	2715.627912	17.583975	-0.051549	2.882587
267.981836	2707.664397	17.588979	-0.051560	2.878696
268.111681	2699.669561	17.593984	-0.051579	2.874787
267.962020	2691.674026	17.598989	-0.051545	2.870857
267.769736	2683.707613	17.603994	-0.051504	2.866933
267.758956	2675.740816	17.608999	-0.051497	2.863014
267.370001	2667.819649	17.614003	-0.051420	2.859092
267.232876	2659.864889	17.619008	-0.051389	2.855161
267.022653	2651.859249	17.624013	-0.051345	2.851195
267.472347	2643.769184	17.629018	-0.051423	2.847219
267.425279	2635.803473	17.634023	-0.051409	2.843271
267.600939	2627.802952	17.639027	-0.051437	2.839313
267.538072	2619.867472	17.644032	-0.051420	2.835368
267.368907	2611.845332	17.649037	-0.051383	2.831369
267.300338	2603.907144	17.654042	-0.051365	2.827412
267.324017	2595.900815	17.659047	-0.051364	2.823420
267.298708	2587.915746	17.664051	-0.051354	2.819430
267.489333	2579.958535	17.669056	-0.051385	2.815461
267.162455	2571.996188	17.674061	-0.051319	2.811455
267.231547	2564.008769	17.679066	-0.051326	2.807452
267.354002	2556.022238	17.684071	-0.051344	2.803448
266.991291	2548.102755	17.689075	-0.051271	2.799443
267.222781	2540.124607	17.694080	-0.051309	2.795437
267.101412	2532.092047	17.699085	-0.051281	2.791378
266.720757	2524.172175	17.704090	-0.051205	2.787355
266.848027	2516.157138	17.709095	-0.051224	2.783307
266.845124	2508.177998	17.714099	-0.051218	2.779264
266.866627	2500.216860	17.719104	-0.051217	2.775226
266.720144	2492.211300	17.724109	-0.051184	2.771149
266.707191	2484.259073	17.729114	-0.051177	2.767101
266.623501	2476.307146	17.734119	-0.051156	2.763044
266.551011	2468.321629	17.739123	-0.051137	2.758964
266.643199	2460.359832	17.744128	-0.051149	2.754899
266.374472	2452.280158	17.749133	-0.051094	2.750747
266.343060	2444.332241	17.754138	-0.051083	2.746670
266.226202	2436.358184	17.759143	-0.051056	2.742569
266.151564	2428.409955	17.764147	-0.051037	2.738477
266.033453	2420.472110	17.769152	-0.051010	2.734382
266.143936	2412.418209	17.774157	-0.051025	2.730235
266.167110	2404.481025	17.779162	-0.051024	2.726136
266.039877	2396.529566	17.784167	-0.050995	2.722015
265.926519	2388.558468	17.789171	-0.050969	2.717878
266.145367	2380.561873	17.794176	-0.051004	2.713742
265.970722	2372.563580	17.799181	-0.050967	2.709575
265.870791	2364.618522	17.804186	-0.050943	2.705433
265.786174	2356.654533	17.809191	-0.050922	2.701276
265.477836	2348.717076	17.814195	-0.050859	2.697112
265.538758	2340.720941	17.819200	-0.050866	2.692935
265.544567	2332.700312	17.824205	-0.050861	2.688735
265.564745	2324.758280	17.829210	-0.050860	2.684570
265.442026	2316.804799	17.834215	-0.050832	2.680383
265.423989	2308.830433	17.839219	-0.050823	2.676186
265.247386	2300.845129	17.844224	-0.050785	2.671967
265.035406	2292.869729	17.849229	-0.050741	2.667743
265.022165	2284.880035	17.854234	-0.050733	2.663518
264.952417	2276.926969	17.859239	-0.050715	2.659302
264.939206	2268.958502	17.864243	-0.050707	2.655075
264.797993	2260.989256	17.869248	-0.050676	2.650832
264.585646	2253.029216	17.874253	-0.050631	2.646583
264.462486	2245.074107	17.879258	-0.050603	2.642335
264.639787	2237.076674	17.884263	-0.050631	2.638078
264.542220	2229.077608	17.889267	-0.050607	2.633795
264.796385	2221.072883	17.894272	-0.050649	2.629525
264.541199	2213.129112	17.899277	-0.050597	2.625247
264.455734	2205.182755	17.904282	-0.050576	2.620972
264.405684	2197.215769	17.909287	-0.050561	2.616681
264.259176	2189.269745	17.914291	-0.050529	2.612388
264.052693	2181.325801	17.919296	-0.050485	2.608085
263.957317	2173.329404	17.924301	-0.050462	2.603753
264.158681	2165.327950	17.929306	-0.050494	2.599432
263.996062	2157.396722	17.934311	-0.050459	2.595118
263.716829	2149.249974	17.939315	-0.050401	2.590670
263.860665	2141.285170	17.944320	-0.050423	2.586343
263.846975	2133.326404	17.949325	-0.050415	2.582002
263.826886	2125.406953	17.954330	-0.050406	2.577674
263.824817	2117.428723	17.959335	-0.050401	2.573308
263.702748	2109.468850	17.964339	-0.050373	2.568936
263.655102	2101.533406	17.969344	-0.050359	2.564575
263.385027	2093.607162	17.974349	-0.050303	2.560197
263.273862	2085.675730	17.979354	-0.050278	2.555819
263.178826	2077.694592	17.984359	-0.050255	2.551407
263.277039	2069.650401	17.989363	-0.050268	2.546967
263.339453	2061.714820	17.994368	-0.050274	2.542576
263.291042	2053.735843	17.999373	-0.050260	2.538146
263.406345	2045.771907	18.004378	-0.050276	2.533728
263.175290	2037.812360	18.009383	-0.050228	2.529280
263.173414	2029.846409	18.014387	-0.050222	2.524837
263.260393	2021.906023	18.019392	-0.050233	2.520406
262.830830	2013.984830	18.024397	-0.050148	2.515942
262.763204	2005.994342	18.029402	-0.050131	2.511457
263.019251	1997.931124	18.034407	-0.050173	2.506946
263.002880	1989.982370	18.039411	-0.050165	2.502472
262.884523	1982.062337	18.044416	-0.050138	2.497998
262.549630	1974.136674	18.049421	-0.050070	2.493498
262.734064	1966.122138	18.054426	-0.050099	2.488977
262.646348	1958.175090	18.059431	-0.050078	2.484466
262.484927	1950.223497	18.064435	-0.050042	2.479939
262.525603	1942.278421	18.069440	-0.050045	2.475422
262.531584	1934.260918	18.074445	-0.050041	2.470854
262.505093	1926.306704	18.079450	-0.050031	2.466310
262.578505	1918.342702	18.084455	-0.050039	2.461760
262.556190	1910.378093	18.089459	-0.050030	2.457194
262.384530	1902.447522	18.094464	-0.049993	2.452627
262.183471	1894.473310	18.099469	-0.049950	2.448025
262.232079	1886.515073	18.104474	-0.049954	2.443443
261.926513	1878.616286	18.109479	-0.049892	2.438859
261.741630	1870.661419	18.114483	-0.049852	2.434243
261.975513	1862.568191	18.119488	-0.049890	2.429570
262.007553	1854.590547	18.124493	-0.049891	2.424939
261.955712	1846.663300	18.129498	-0.049876	2.420323
261.660492	1838.757940	18.134503	-0.049816	2.415692
261.574063	1830.780219	18.139507	-0.049795	2.411026
261.178318	1822.890153	18.144512	-0.049716	2.406378
261.227824	1814.884947	18.149517	-0.049720	2.401688
261.636591	1806.871220	18.154522	-0.049791	2.397012
261.230319	1798.972318	18.159527	-0.049710	2.392331
261.295926	1790.955113	18.164531	-0.049717	2.387608
261.282337	1783.004929	18.169536	-0.049709	2.382909
261.322325	1775.039301	18.174541	-0.049712	2.378195
261.358870	1767.091992	18.179546	-0.049713	2.373483
261.433578	1759.116755	18.184551	-0.049722	2.368748
261.093372	1751.219653	18.189555	-0.049654	2.364017
261.134493	1743.267190	18.194560	-0.049656	2.359273
260.946957	1735.321574	18.199565	-0.049616	2.354506
260.943292	1727.328081	18.204570	-0.049610	2.349715
260.784959	1719.377478	18.209575	-0.049575	2.344928
260.791384	1711.405121	18.214579	-0.049571	2.340131
260.723353	1703.477797	18.219584	-0.049554	2.335346
260.410415	1695.522285	18.224589	-0.049490	2.330513
260.487664	1687.554695	18.229594	-0.049499	2.325695
260.510837	1679.610392	18.234599	-0.049498	2.320877
260.203429	1671.698856	18.239603	-0.049436	2.316042
260.357287	1663.692501	18.244608	-0.049459	2.311176
260.228999	1655.728145	18.249613	-0.049430	2.306303
260.185050	1647.799235	18.254618	-0.049417	2.301448
260.187311	1639.863960	18.259623	-0.049412	2.296582
260.116171	1631.874348	18.264627	-0.049394	2.291667
260.342835	1623.905071	18.269632	-0.049431	2.286779
260.121512	1615.986994	18.274637	-0.049384	2.281874
260.036391	1608.062279	18.279642	-0.049363	2.276966
259.987243	1600.061927	18.284647	-0.049349	2.272003
259.936461	1592.071770	18.289651	-0.049334	2.267036
259.688365	1584.183301	18.294656	-0.049283	2.262104
259.657701	1576.223589	18.299661	-0.049272	2.257136
259.750811	1568.253019	18.304666	-0.049284	2.252161
259.523506	1560.337274	18.309671	-0.049237	2.247181
259.486776	1552.374476	18.314675	-0.049225	2.242177
259.523841	1544.450648	18.319680	-0.049227	2.237193
259.413454	1536.483931	18.324685	-0.049201	2.232157
259.327044	1528.545962	18.329690	-0.049180	2.227131
259.280292	1520.601957	18.334695	-0.049166	2.222093
259.131690	1512.663003	18.339699	-0.049133	2.217037
259.172265	1504.701997	18.344704	-0.049135	2.211973
259.093964	1496.752414	18.349709	-0.049115	2.206894
259.086153	1488.812965	18.354714	-0.049109	2.201816
258.937473	1480.903636	18.359719	-0.049076	2.196732
258.879852	1472.921475	18.364723	-0.049060	2.191599
258.949853	1464.943893	18.369728	-0.049068	2.186468
258.745080	1457.027936	18.374733	-0.049025	2.181339
258.625077	1449.113902	18.379738	-0.048997	2.176207
258.425266	1441.180160	18.384743	-0.048955	2.171044
258.466266	1433.202207	18.389747	-0.048957	2.165861
258.315530	1425.304062	18.394752	-0.048924	2.160700
258.207654	1417.368655	18.399757	-0.048899	2.155506
258.313864	1409.382624	18.404762	-0.048913	2.150286
258.163050	1401.461848	18.409767	-0.048880	2.145073
258.143409	1393.519394	18.414771	-0.048871	2.139845
258.346940	1385.564870	18.419776	-0.048904	2.134617
258.138152	1377.628413	18.424781	-0.048860	2.129349
258.002948	1369.716220	18.429786	-0.048829	2.124092
258.107107	1361.769819	18.434791	-0.048844	2.118821
257.969427	1353.831802	18.439795	-0.048813	2.113519
257.943699	1345.846760	18.444800	-0.048803	2.108184
257.748314	1337.920621	18.449805	-0.048761	2.102858
257.819522	1329.987542	18.454810	-0.048769	2.097540
257.846021	1322.043450	18.459815	-0.048769	2.092196
257.397997	1314.149554	18.464819	-0.048681	2.086826
257.464550	1306.229057	18.469824	-0.048688	2.081475
257.290618	1298.304031	18.474829	-0.048650	2.076083
257.123612	1290.361095	18.479834	-0.048614	2.070666
257.216969	1282.402266	18.484839	-0.048626	2.065249
257.258721	1274.463996	18.489843	-0.048629	2.059827
257.228386	1266.567793	18.494848	-0.048618	2.054412
257.130387	1258.617230	18.499853	-0.048595	2.048939
257.081030	1250.706633	18.504858	-0.048580	2.043484
257.088903	1242.769745	18.509863	-0.048577	2.038001
256.958509	1234.830828	18.514867	-0.048547	2.032489
256.939752	1226.897563	18.519872	-0.048538	2.026976
256.606011	1219.002026	18.524877	-0.048471	2.021443
256.665575	1211.072152	18.529882	-0.048477	2.015911
256.571739	1203.137425	18.534887	-0.048454	2.010344
256.526356	1195.206687	18.539891	-0.048441	2.004770
256.432454	1187.313166	18.544896	-0.048418	1.999201
256.140343	1179.410139	18.549901	-0.048359	1.993589
256.255070	1171.445872	18.554906	-0.048375	1.987961
256.227396	1163.522784	18.559911	-0.048364	1.982331
256.077176	1155.619421	18.564915	-0.048331	1.976686
256.065884	1147.694247	18.569920	-0.048324	1.971024
255.925814	1139.765121	18.574925	-0.048293	1.965329
255.923717	1131.862323	18.579930	-0.048287	1.959651
255.773665	1123.963424	18.584935	-0.048254	1.953943
255.549804	1115.999530	18.589939	-0.048207	1.948164
255.677898	1108.063428	18.594944	-0.048226	1.942426
255.634052	1100.150294	18.599949	-0.048213	1.936669
255.544578	1092.234204	18.604954	-0.048191	1.930887
255.536139	1084.309635	18.609959	-0.048184	1.925091
255.494581	1076.408586	18.614963	-0.048171	1.919291
255.607138	1068.488043	18.619968	-0.048187	1.913476
255.416586	1060.573462	18.624973	-0.048146	1.907614
255.396006	1052.674468	18.629978	-0.048137	1.901765
255.123575	1044.807263	18.634983	-0.048082	1.895892
255.096274	1036.860077	18.639987	-0.048071	1.889970
255.155021	1028.961435	18.644992	-0.048077	1.884075
254.820085	1021.093225	18.649997	-0.048010	1.878139
254.682313	1013.188620	18.655002	-0.047979	1.872179
254.771021	1005.233216	18.660007	-0.047990	1.866189
254.669233	997.332318	18.665011	-0.047966	1.860198
254.557861	989.467625	18.670016	-0.047940	1.854214
254.524084	981.529137	18.675021	-0.047929	1.848164
254.599254	973.616668	18.680026	-0.047937	1.842126
254.329583	965.761792	18.685031	-0.047882	1.836072
254.234488	957.842391	18.690035	-0.047859	1.829969
254.214969	949.939851	18.695040	-0.047851	1.823867
254.064616	942.059527	18.700045	-0.047817	1.817747
253.989041	934.154397	18.705050	-0.047798	1.811596
253.920646	926.256248	18.710055	-0.047780	1.805430
253.758544	918.387034	18.715059	-0.047745	1.799254
253.830597	910.474368	18.720064	-0.047753	1.793051
253.671799	902.544231	18.725069	-0.047718	1.786784
253.701176	894.646135	18.730074	-0.047719	1.780544
253.528622	886.791502	18.735079	-0.047682	1.774292
253.463235	878.879694	18.740083	-0.047664	1.767985
253.380470	871.023021	18.745088	-0.047644	1.761697
253.043412	863.176939	18.750093	-0.047576	1.755364
253.158944	855.237489	18.755098	-0.047592	1.748989
253.360445	847.309145	18.760103	-0.047624	1.742611
252.989144	839.486146	18.765107	-0.047550	1.736222
253.003991	831.592684	18.770112	-0.047548	1.729801
252.931073	823.714567	18.775117	-0.047529	1.723358
252.723833	815.874482	18.780122	-0.047485	1.716904
252.709639	807.969859	18.785127	-0.047478	1.710398
252.626717	800.075535	18.790131	-0.047457	1.703866
252.457222	792.237556	18.795136	-0.047420	1.697345
252.265772	784.362337	18.800141	-0.047380	1.690765
252.303828	776.477358	18.805146	-0.047382	1.684181
252.174407	768.627140	18.810151	-0.047352	1.677578
251.978104	760.761153	18.815155	-0.047311	1.670926
251.983924	752.887016	18.820160	-0.047307	1.664269
251.940485	745.022049	18.825165	-0.047293	1.657586
252.131060	737.116676	18.830170	-0.047324	1.650872
251.896852	729.286967	18.835175	-0.047275	1.644139
251.774792	721.451883	18.840179	-0.047247	1.637388
251.701328	713.549904	18.845184	-0.047228	1.630559
251.362274	705.705493	18.850189	-0.047160	1.623713
251.282058	697.861466	18.855194	-0.047140	1.616875
251.348723	689.983633	18.860199	-0.047147	1.609999
251.212397	682.137606	18.865203	-0.047117	1.603093
251.308166	674.290332	18.870208	-0.047130	1.596189
251.192322	666.430796	18.875213	-0.047103	1.589214
250.907641	658.627903	18.880218	-0.047045	1.582234
250.546401	650.842191	18.885223	-0.046972	1.575227
250.554705	642.954424	18.890227	-0.046969	1.568151
250.661552	635.100947	18.895232	-0.046984	1.561088
250.408607	627.302788	18.900237	-0.046931	1.553990
250.052112	619.485987	18.905242	-0.046860	1.546828
250.280872	611.591620	18.910247	-0.046897	1.539648
249.992633	603.787241	18.915251	-0.046839	1.532440
250.081825	595.933031	18.920256	-0.046850	1.525208
249.986656	588.117128	18.925261	-0.046827	1.517950
250.073598	580.261993	18.930266	-0.046838	1.510648
250.047437	572.438121	18.935271	-0.046828	1.503322
249.677320	564.673675	18.940275	-0.046754	1.495964
249.316679	556.911296	18.945280	-0.046682	1.488572
249.494481	549.032355	18.950285	-0.046710	1.481116
249.249299	541.254370	18.955290	-0.046660	1.473653
249.141271	533.399859	18.960295	-0.046634	1.466100
249.099233	525.591165	18.965299	-0.046621	1.458563
249.059713	517.789123	18.970304	-0.046609	1.450993
248.917645	509.996837	18.975309	-0.046577	1.443377
248.900999	502.208883	18.980314	-0.046569	1.435744
248.787917	494.413502	18.985319	-0.046543	1.428048
248.599530	486.636289	18.990323	-0.046503	1.420316
248.694233	478.839286	18.995328	-0.046515	1.412568
248.552270	471.054321	19.000333	-0.046484	1.404750
248.430110	463.300198	19.005338	-0.046456	1.396923
248.315434	455.518681	19.010343	-0.046430	1.389026
248.221653	447.732880	19.015347	-0.046407	1.381082
248.167470	439.980879	19.020352	-0.046392	1.373134
247.772399	432.242644	19.025357	-0.046313	1.365095
247.873816	424.465873	19.030362	-0.046327	1.357054
247.907314	416.685328	19.035367	-0.046328	1.348949
247.518751	408.966475	19.040371	-0.046251	1.340786
247.693551	401.189194	19.045376	-0.046279	1.332611
247.251740	393.488926	19.050381	-0.046191	1.324358
247.230274	385.753305	19.055386	-0.046182	1.316090
247.002147	377.900591	19.060391	-0.046135	1.307606
247.105535	370.137158	19.065395	-0.046149	1.299224
246.736218	362.473189	19.070400	-0.046075	1.290810
246.657002	354.740278	19.075405	-0.046055	1.282318
246.644618	347.029512	19.080410	-0.046048	1.273807
246.340463	339.341343	19.085415	-0.045986	1.265208
246.108940	331.657989	19.090419	-0.045938	1.256570
246.144034	323.937818	19.095424	-0.045940	1.247881
246.078699	316.243460	19.100429	-0.045922	1.239141
245.824197	308.575564	19.105434	-0.045870	1.230333
245.809035	300.865204	19.110439	-0.045862	1.221458
245.750566	293.177654	19.115443	-0.045846	1.212537
245.566968	285.529335	19.120448	-0.045807	1.203571
245.262543	277.903460	19.125453	-0.045746	1.194540
245.105184	270.243308	19.130458	-0.045711	1.185428
244.952168	262.607103	19.135463	-0.045678	1.176276
244.775098	254.957287	19.140467	-0.045640	1.167030
244.699636	247.327015	19.145472	-0.045621	1.157756
244.438160	239.675781	19.150477	-0.045567	1.148341
243.955041	232.115753	19.155482	-0.045472	1.138915
243.689917	224.511157	19.160487	-0.045418	1.129401
243.464093	216.913472	19.165491	-0.045371	1.119822
243.179511	209.336895	19.170496	-0.045313	1.110176
242.749414	201.777886	19.175501	-0.045228	1.100435
242.442116	194.216767	19.180506	-0.045166	1.090631
241.942264	186.699457	19.185511	-0.045068	1.080752
241.233042	179.202584	19.190515	-0.044931	1.070761
240.868183	171.657383	19.195520	-0.044858	1.060690
240.278066	164.158545	19.200525	-0.044743	1.050533
239.869433	156.642362	19.205530	-0.044662	1.040295
239.434979	149.145562	19.210535	-0.044576	1.029976
238.997260	141.645952	19.215539	-0.044490	1.019547
238.497988	134.187403	19.220544	-0.044392	1.009052
238.030611	126.725718	19.225549	-0.044300	0.998451
237.569759	119.241155	19.230554	-0.044210	0.987704
237.066851	111.811099	19.235559	-0.044111	0.976908
236.538764	104.381516	19.240563	-0.044008	0.965984
236.070733	96.986918	19.245568	-0.043916	0.955002
235.629751	89.573718	19.250573	-0.043829	0.943872
235.125255	82.200738	19.255578	-0.043730	0.932652
234.460447	74.866296	19.260583	-0.043602	0.921312
233.791268	67.538351	19.265587	-0.043472	0.909839
233.338874	60.428925	19.270592	-0.043384	0.898622