Tue Mar 23 10:48:27 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.844412	-0.044870	0.000000	-0.000044	0.721142

0.981639	-0.069967	0.005005	-0.000070	0.721141
0.736506	-0.029687	0.010010	-0.000024	0.721134
0.875210	-0.051120	0.015014	-0.000050	0.721140
0.527194	0.013903	0.020019	0.000015	0.721146
0.812141	-0.039239	0.025024	-0.000038	0.721142
1.199564	-0.113482	0.030029	-0.000110	0.721131
1.129033	-0.104089	0.035034	-0.000097	0.721125
1.094165	-0.092239	0.040038	-0.000091	0.721136
0.910698	-0.062938	0.045043	-0.000057	0.721129
0.923493	-0.060883	0.050048	-0.000059	0.721138
1.108622	-0.195604	0.055053	-0.000093	0.720938
0.972435	-0.202437	0.060058	-0.000068	0.720876
1.023917	-0.207351	0.065062	-0.000078	0.720885
0.887301	-0.186865	0.070067	-0.000052	0.720877
1.015282	-0.207977	0.075072	-0.000076	0.720880
1.163425	-0.233035	0.080077	-0.000103	0.720883
1.146243	-0.231276	0.085082	-0.000100	0.720880
1.189116	-0.401914	0.090086	-0.000108	0.720560
1.036031	-0.384280	0.095091	-0.000080	0.720541
1.042611	-0.381440	0.100096	-0.000081	0.720548
1.102930	-0.393439	0.105101	-0.000092	0.720546
1.135172	-0.401944	0.110106	-0.000098	0.720540
1.023169	-0.531342	0.115110	-0.000077	0.720246
1.127436	-0.561902	0.120115	-0.000096	0.720223
0.988856	-0.532584	0.125120	-0.000071	0.720232
0.950495	-0.525626	0.130125	-0.000064	0.720232
0.919152	-0.626351	0.135130	-0.000058	0.720023
1.049178	-0.705570	0.140134	-0.000082	0.719912
0.831190	-0.670311	0.145139	-0.000041	0.719905
0.698316	-0.645020	0.150144	-0.000016	0.719908
0.682031	-0.747745	0.155149	-0.000013	0.719700
0.855672	-0.829163	0.160154	-0.000046	0.719600
0.767087	-0.806850	0.165158	-0.000029	0.719613
0.827070	-0.844476	0.170163	-0.000040	0.719560
0.925764	-1.005409	0.175168	-0.000059	0.719277
0.974668	-1.014029	0.180173	-0.000068	0.719277
0.913062	-1.005147	0.185178	-0.000056	0.719273
0.951626	-1.166627	0.190182	-0.000063	0.718968
0.803718	-1.142495	0.195187	-0.000036	0.718964
0.828356	-1.151856	0.200192	-0.000040	0.718954
0.837253	-1.305731	0.205197	-0.000042	0.718653
0.575953	-1.260102	0.210202	0.000007	0.718652
0.771362	-1.324100	0.215206	-0.000029	0.718594
0.776676	-1.443439	0.220211	-0.000030	0.718360
0.597794	-1.409284	0.225216	0.000003	0.718365
0.677429	-1.515195	0.230221	-0.000012	0.718183
0.475506	-1.560991	0.235226	0.000026	0.718022
0.607296	-1.580936	0.240230	0.000001	0.718029
0.204130	-1.663128	0.245235	0.000076	0.717724
0.313399	-1.684907	0.250240	0.000056	0.717720
0.666461	-1.817483	0.255245	-0.000010	0.717582
0.429677	-1.875193	0.260250	0.000035	0.717384
0.550512	-1.899741	0.265254	0.000012	0.717378
0.497735	-2.038511	0.270259	0.000022	0.717085
0.613434	-2.056188	0.275264	0.000001	0.717091
0.324214	-2.136389	0.280269	0.000054	0.716830
0.300438	-2.168418	0.285274	0.000059	0.716758
0.274311	-2.247445	0.290278	0.000064	0.716593
0.006079	-2.268439	0.295283	0.000114	0.716457
0.157671	-2.350989	0.300288	0.000086	0.716347
0.040549	-2.430660	0.305293	0.000107	0.716147
-0.186228	-2.422443	0.310298	0.000150	0.716084
-1.355405	-2.311355	0.315302	0.000367	0.715891
-1.996938	-2.198307	0.320307	0.000487	0.715889
-2.489348	-2.205753	0.325312	0.000578	0.715700
-3.036073	-2.181420	0.330317	0.000680	0.715555
-2.923841	-2.204116	0.335322	0.000659	0.715550
-2.993062	-2.255804	0.340326	0.000672	0.715423
-3.890154	-2.190278	0.345331	0.000839	0.715236
-3.818831	-2.198606	0.350336	0.000826	0.715244
-4.175135	-2.136590	0.355341	0.000892	0.715242
-4.603580	-2.212864	0.360346	0.000972	0.714939
-4.565955	-2.231431	0.365350	0.000965	0.714915
-5.095102	-2.140318	0.370355	0.001064	0.714909
-4.933883	-2.168474	0.375360	0.001034	0.714910
-5.097109	-2.278354	0.380365	0.001064	0.714634
-5.665356	-2.190571	0.385370	0.001170	0.714607
-5.782050	-2.164903	0.390374	0.001192	0.714617
-5.447491	-2.228966	0.395379	0.001129	0.714608
-6.149829	-2.223899	0.400384	0.001260	0.714370
-6.789229	-2.152543	0.405389	0.001379	0.714285
-6.925782	-2.131235	0.410394	0.001405	0.714279
-6.352921	-2.225057	0.415398	0.001298	0.714295
-6.689962	-2.170709	0.420403	0.001361	0.714284
-7.130816	-2.225156	0.425408	0.001443	0.714020
-7.633452	-2.155089	0.430413	0.001536	0.713981
-7.876357	-2.115346	0.435418	0.001582	0.713974
-7.571910	-2.167251	0.440422	0.001525	0.713979
-7.758926	-2.133576	0.445427	0.001560	0.713979
-7.646918	-2.216533	0.450432	0.001539	0.713854
-8.667302	-2.128652	0.455437	0.001729	0.713667
-8.663228	-2.134000	0.460442	0.001728	0.713658
-8.643228	-2.131274	0.465446	0.001725	0.713671
-8.561509	-2.150296	0.470451	0.001709	0.713662
-8.835161	-2.102090	0.475456	0.001760	0.713661
-8.829314	-2.127690	0.480461	0.001759	0.713612
-9.447955	-2.140171	0.485466	0.001874	0.713368
-9.358133	-2.152514	0.490470	0.001858	0.713375
-9.773523	-2.083021	0.495475	0.001935	0.713366
-9.294912	-2.165327	0.500480	0.001846	0.713372
-9.282063	-2.162547	0.505485	0.001844	0.713382
-10.005337	-2.035776	0.510490	0.001978	0.713378
-9.723518	-2.227559	0.515494	0.001926	0.713096
-10.673365	-2.082970	0.520499	0.002103	0.713047
-10.836629	-2.056740	0.525504	0.002133	0.713041
-10.037625	-2.198712	0.530509	0.001984	0.713042
-10.103342	-2.194093	0.535514	0.001997	0.713028
-10.433594	-2.131528	0.540518	0.002058	0.713035
-10.589631	-2.160063	0.545523	0.002087	0.712923
-11.343651	-2.125410	0.550528	0.002227	0.712725
-10.902011	-2.201333	0.555533	0.002145	0.712730
-11.726333	-2.059376	0.560538	0.002299	0.712720
-11.374910	-2.120285	0.565542	0.002233	0.712724
-10.920840	-2.205438	0.570547	0.002149	0.712715
-11.640824	-2.076463	0.575552	0.002283	0.712717
-11.578175	-2.176019	0.580557	0.002271	0.712541
-12.408393	-2.100038	0.585562	0.002426	0.712397
-12.122352	-2.144758	0.590566	0.002373	0.712410
-12.518807	-2.075649	0.595571	0.002446	0.712407
-12.564934	-2.066365	0.600576	0.002455	0.712409
-12.255954	-2.124182	0.605581	0.002397	0.712403
-12.636194	-2.060077	0.610586	0.002468	0.712396
-12.434877	-2.122960	0.615590	0.002431	0.712342
-12.926232	-2.157840	0.620595	0.002522	0.712098
-13.179816	-2.109522	0.625600	0.002570	0.712104
-13.512418	-2.045208	0.630605	0.002631	0.712115
-13.014473	-2.140409	0.635610	0.002539	0.712102
-12.940299	-2.152204	0.640614	0.002525	0.712104
-13.464270	-2.060768	0.645619	0.002622	0.712101
-13.275070	-2.124692	0.650624	0.002587	0.712040
-13.579106	-2.205332	0.655629	0.002644	0.711771
-14.322447	-2.075124	0.660634	0.002782	0.711767
-14.164118	-2.098117	0.665638	0.002753	0.711777
-13.796267	-2.167008	0.670643	0.002684	0.711771
-14.021582	-2.126780	0.675648	0.002726	0.711771
-14.308488	-2.071704	0.680653	0.002780	0.711779
-14.156751	-2.130976	0.685658	0.002752	0.711714
-14.767397	-2.145072	0.690662	0.002865	0.711469
-15.272975	-2.054168	0.695667	0.002959	0.711471
-15.262147	-2.057926	0.700672	0.002957	0.711467
-14.715319	-2.151193	0.705677	0.002856	0.711476
-15.131993	-2.082857	0.710682	0.002933	0.711464
-14.922064	-2.118489	0.715686	0.002894	0.711467
-14.741282	-2.157729	0.720691	0.002860	0.711453
-15.495697	-2.178383	0.725696	0.003001	0.711144
-16.083449	-2.071859	0.730701	0.003110	0.711147
-16.166533	-2.059550	0.735706	0.003126	0.711142
-15.417372	-2.187345	0.740710	0.002986	0.711154
-15.723070	-2.136703	0.745715	0.003043	0.711146
-15.972226	-2.091483	0.750720	0.003090	0.711148
-15.596452	-2.173750	0.755725	0.003020	0.711117
-16.616370	-2.114503	0.760730	0.003210	0.710873
-16.725930	-2.090127	0.765734	0.003230	0.710882
-16.641502	-2.108835	0.770739	0.003214	0.710875
-16.557498	-2.121330	0.775744	0.003199	0.710880
-16.626938	-2.106604	0.780749	0.003212	0.710884
-16.815457	-2.078479	0.785754	0.003247	0.710874
-16.588990	-2.147741	0.790758	0.003205	0.710816
-17.637470	-2.099910	0.795763	0.003400	0.710538
-17.651258	-2.097249	0.800768	0.003402	0.710539
-17.498093	-2.121209	0.805773	0.003374	0.710545
-17.654055	-2.098608	0.810778	0.003403	0.710535
-17.461753	-2.127002	0.815782	0.003367	0.710546
-17.513492	-2.119923	0.820787	0.003377	0.710542
-17.451644	-2.164724	0.825792	0.003365	0.710475
-18.272663	-2.142939	0.830797	0.003518	0.710226
-18.391585	-2.123654	0.835802	0.003540	0.710222
-18.318763	-2.130919	0.840806	0.003527	0.710233
-18.320511	-2.134426	0.845811	0.003527	0.710226
-18.524523	-2.099082	0.850816	0.003565	0.710224
-18.405108	-2.115313	0.855821	0.003543	0.710234
-18.399870	-2.179216	0.860826	0.003542	0.710108
-19.452215	-2.089837	0.865830	0.003738	0.709912
-19.240063	-2.131884	0.870835	0.003698	0.709903
-19.814356	-2.026074	0.875840	0.003805	0.709910
-19.794656	-2.024384	0.880845	0.003802	0.709921
-19.558717	-2.073713	0.885850	0.003758	0.709906
-19.412734	-2.094798	0.890854	0.003731	0.709916
-19.812792	-2.022531	0.895859	0.003805	0.709918
-19.971897	-2.082212	0.900864	0.003835	0.709742
-20.549016	-2.041055	0.905869	0.003942	0.709618
-20.315915	-2.089681	0.910874	0.003899	0.709604
-20.357168	-2.079825	0.915878	0.003906	0.709609
-20.671779	-2.024772	0.920883	0.003965	0.709607
-20.579804	-2.038069	0.925888	0.003948	0.709613
-20.397040	-2.068285	0.930893	0.003914	0.709618
-20.767427	-2.005595	0.935898	0.003983	0.709611
-20.958545	-2.110815	0.940902	0.004018	0.709332
-21.478175	-2.047032	0.945907	0.004115	0.709275
-21.734839	-1.998364	0.950912	0.004163	0.709281
-20.808325	-2.164423	0.955917	0.003991	0.709279
-21.404552	-2.058018	0.960922	0.004102	0.709279
-21.590405	-2.017561	0.965926	0.004136	0.709294
-21.127158	-2.103958	0.970931	0.004050	0.709286
-21.473639	-2.131298	0.975936	0.004114	0.709108
-22.947731	-1.924050	0.980941	0.004389	0.708997
-23.007866	-1.918080	0.985946	0.004400	0.708987
-22.935589	-1.921206	0.990950	0.004387	0.709007
-23.076148	-1.896229	0.995955	0.004413	0.709006
-23.145073	-1.888031	1.000960	0.004426	0.708998
-22.762504	-1.953581	1.005965	0.004354	0.709004
-22.396063	-2.033250	1.010970	0.004286	0.708975
-22.179162	-2.073801	1.015974	0.004246	0.708971
-22.539762	-2.104466	1.020979	0.004313	0.708781
-23.419498	-2.011744	1.025984	0.004477	0.708652
-23.071026	-2.069663	1.030989	0.004412	0.708661
-23.404278	-2.008907	1.035994	0.004474	0.708664
-23.204267	-2.044032	1.040998	0.004437	0.708665
-23.173358	-2.045908	1.046003	0.004431	0.708672
-23.306738	-2.026650	1.051008	0.004456	0.708663
-23.362940	-2.127325	1.056013	0.004466	0.708441
-23.898429	-2.070524	1.061018	0.004566	0.708364
-24.058477	-2.039503	1.066022	0.004596	0.708368
-24.028215	-2.046561	1.071027	0.004590	0.708365
-24.078568	-2.036995	1.076032	0.004600	0.708366
-23.951197	-2.053725	1.081037	0.004576	0.708378
-24.394693	-1.990495	1.086042	0.004659	0.708347
-24.671694	-2.096066	1.091046	0.004710	0.708036
-24.970793	-2.040655	1.096051	0.004766	0.708040
-25.330020	-1.978966	1.101056	0.004833	0.708035
-24.982318	-2.038817	1.106061	0.004768	0.708040
-24.863424	-2.067351	1.111066	0.004746	0.708025
-24.999371	-2.038018	1.116070	0.004771	0.708035
-24.880564	-2.066731	1.121075	0.004749	0.708020
-25.267757	-2.149362	1.126080	0.004821	0.707716
-25.572271	-2.093569	1.131085	0.004878	0.707719
-26.136088	-1.997091	1.136090	0.004983	0.707711
-25.697199	-2.073856	1.141094	0.004901	0.707714
-25.629004	-2.085027	1.146099	0.004889	0.707716
-26.171191	-1.990342	1.151104	0.004989	0.707712
-25.874155	-2.074893	1.156109	0.004934	0.707648
-26.615283	-2.072705	1.161114	0.005072	0.707388
-26.578164	-2.071107	1.166118	0.005065	0.707404
-27.008349	-1.998362	1.171123	0.005145	0.707396
-26.996416	-2.004445	1.176128	0.005143	0.707388
-26.316858	-2.118970	1.181133	0.005017	0.707401
-26.727206	-2.055126	1.186138	0.005093	0.707383
-26.811630	-2.061379	1.191142	0.005109	0.707340
-27.423699	-2.071829	1.196147	0.005223	0.707100
-27.749000	-2.012798	1.201152	0.005283	0.707102
-27.388221	-2.077551	1.206157	0.005216	0.707101
-27.718498	-2.016933	1.211162	0.005278	0.707105
-27.351352	-2.085659	1.216166	0.005209	0.707098
-27.668814	-2.027324	1.221171	0.005268	0.707102
-27.555165	-2.103029	1.226176	0.005247	0.706990
-27.962864	-2.138883	1.231181	0.005323	0.706772
-28.527492	-2.044423	1.236186	0.005428	0.706760
-28.690615	-2.011652	1.241190	0.005459	0.706767
-28.236916	-2.092812	1.246195	0.005374	0.706767
-28.228507	-2.094029	1.251200	0.005373	0.706767
-28.585836	-2.028318	1.256205	0.005439	0.706771
-28.504177	-2.117365	1.261210	0.005424	0.706622
-29.214864	-2.073570	1.266214	0.005556	0.706455
-29.360756	-2.047832	1.271219	0.005584	0.706454
-29.748879	-1.979932	1.276224	0.005656	0.706452
-28.890297	-2.130301	1.281229	0.005496	0.706457
-29.257438	-2.067888	1.286234	0.005564	0.706451
-29.460971	-2.028965	1.291238	0.005602	0.706456
-29.384776	-2.116577	1.296243	0.005588	0.706308
-30.324974	-2.035290	1.301248	0.005763	0.706134
-29.960948	-2.097637	1.306253	0.005695	0.706139
-30.354123	-2.032794	1.311258	0.005769	0.706129
-30.097708	-2.076040	1.316262	0.005721	0.706133
-30.059888	-2.081102	1.321267	0.005714	0.706137
-30.378902	-2.024547	1.326272	0.005773	0.706136
-29.965661	-2.176347	1.331277	0.005696	0.705979
-31.217887	-2.010772	1.336282	0.005929	0.705863
-31.065524	-2.032914	1.341286	0.005901	0.705873
-30.783505	-2.082588	1.346291	0.005849	0.705874
-30.965835	-2.049461	1.351296	0.005883	0.705876
-30.772122	-2.084637	1.356301	0.005847	0.705874
-31.002827	-2.045023	1.361306	0.005889	0.705871
-31.456758	-2.118872	1.366310	0.005974	0.705560
-31.698799	-2.090303	1.371315	0.006019	0.705530
-32.059046	-2.026202	1.376320	0.006086	0.705530
-31.469083	-2.126808	1.381325	0.005976	0.705539
-31.953033	-2.042055	1.386330	0.006066	0.705536
-31.809326	-2.068396	1.391334	0.006040	0.705535
-31.675482	-2.129157	1.396339	0.006015	0.705461
-32.743309	-2.060547	1.401344	0.006214	0.705215
-32.613826	-2.079160	1.406349	0.006190	0.705224
-32.918939	-2.028993	1.411354	0.006246	0.705216
-32.721863	-2.062095	1.416358	0.006210	0.705220
-32.669307	-2.073663	1.421363	0.006200	0.705216
-33.343098	-1.947280	1.426368	0.006325	0.705228
-32.942054	-2.016155	1.431373	0.006251	0.705233
-33.306840	-2.098885	1.436378	0.006319	0.704936
-33.937402	-2.000082	1.441382	0.006436	0.704908
-33.753256	-2.034678	1.446387	0.006402	0.704905
-33.515732	-2.084173	1.451392	0.006358	0.704890
-33.713934	-2.040197	1.456397	0.006394	0.704908
-34.111661	-1.968560	1.461402	0.006468	0.704909
-33.947761	-1.995402	1.466406	0.006438	0.704914
-33.963767	-2.044100	1.471411	0.006441	0.704810
-34.896803	-1.974916	1.476416	0.006615	0.704614
-34.285369	-2.078859	1.481421	0.006501	0.704625
-34.805265	-1.992222	1.486426	0.006598	0.704612
-35.023731	-1.947773	1.491430	0.006638	0.704623
-34.432371	-2.057083	1.496435	0.006528	0.704616
-34.946103	-1.966278	1.501440	0.006624	0.704614
-35.296330	-1.892729	1.506445	0.006689	0.704636
-35.070988	-2.077764	1.511450	0.006647	0.704344
-35.567429	-2.025223	1.516454	0.006740	0.704272
-35.554220	-2.025517	1.521459	0.006737	0.704276
-35.690174	-1.999610	1.526464	0.006763	0.704279
-35.553135	-2.020390	1.531469	0.006737	0.704287
-35.253206	-2.083055	1.536474	0.006681	0.704268
-35.268727	-2.080396	1.541478	0.006684	0.704268
-35.580448	-2.172602	1.546483	0.006742	0.703970
-36.259608	-2.054006	1.551488	0.006869	0.703965
-36.550746	-1.996027	1.556493	0.006923	0.703977
-36.311132	-2.046506	1.561498	0.006878	0.703961
-36.121897	-2.081970	1.566502	0.006843	0.703958
-36.242766	-2.059216	1.571507	0.006866	0.703960
-36.289662	-2.112044	1.576512	0.006874	0.703837
-37.098210	-2.060647	1.581517	0.007025	0.703650
-37.022195	-2.079911	1.586522	0.007011	0.703638
-37.550417	-1.985627	1.591526	0.007109	0.703638
-37.056868	-2.072127	1.596531	0.007017	0.703641
-36.967257	-2.091069	1.601536	0.007001	0.703635
-37.182243	-2.047131	1.606541	0.007041	0.703647
-37.348328	-2.099947	1.611546	0.007072	0.703480
-38.029478	-2.040751	1.616550	0.007198	0.703354
-37.777435	-2.083159	1.621555	0.007151	0.703360
-38.034286	-2.047297	1.626560	0.007199	0.703339
-37.865766	-2.071067	1.631565	0.007168	0.703352
-37.886946	-2.070336	1.636570	0.007172	0.703346
-38.125943	-2.026100	1.641574	0.007216	0.703349
-38.228533	-2.161252	1.646579	0.007236	0.703039
-38.880333	-2.061237	1.651584	0.007357	0.703007
-39.053146	-2.023815	1.656589	0.007389	0.703020
-38.980350	-2.039565	1.661594	0.007375	0.703014
-38.894470	-2.053822	1.666598	0.007359	0.703016
-38.917332	-2.050511	1.671603	0.007364	0.703015
-39.229724	-1.998637	1.676608	0.007422	0.703007
-39.020284	-2.165124	1.681613	0.007383	0.702746
-39.712083	-2.065730	1.686618	0.007512	0.702698
-39.915340	-2.028946	1.691622	0.007550	0.702699
-39.579934	-2.086259	1.696627	0.007487	0.702704
-39.626190	-2.081325	1.701632	0.007496	0.702697
-39.446242	-2.110344	1.706637	0.007462	0.702703
-39.594428	-2.138669	1.711642	0.007490	0.702593
-40.621723	-2.061793	1.716646	0.007681	0.702378
-40.392829	-2.098614	1.721651	0.007639	0.702386
-41.112255	-1.973747	1.726656	0.007772	0.702379
-40.482111	-2.081676	1.731661	0.007655	0.702388
-40.263754	-2.125264	1.736666	0.007615	0.702378
-40.629947	-2.058777	1.741670	0.007683	0.702381
-40.925968	-2.063188	1.746675	0.007738	0.702265
-41.737770	-2.012290	1.751680	0.007889	0.702075
-41.222778	-2.095566	1.756685	0.007793	0.702093
-41.723656	-2.004757	1.761690	0.007886	0.702096
-41.415529	-2.062227	1.766694	0.007829	0.702090
-41.348508	-2.069922	1.771699	0.007817	0.702099
-42.102654	-1.937511	1.776704	0.007957	0.702095
-41.754625	-1.999239	1.781709	0.007892	0.702096
-42.029113	-2.110552	1.786714	0.007943	0.701771
-42.413557	-2.046786	1.791718	0.008015	0.701762
-42.598640	-2.016903	1.796723	0.008049	0.701755
-42.278975	-2.079051	1.801728	0.007990	0.701745
-42.232401	-2.078670	1.806733	0.007981	0.701762
-42.819534	-1.975876	1.811738	0.008091	0.701759
-42.580655	-2.019225	1.816742	0.008046	0.701757
-42.551563	-2.154247	1.821747	0.008041	0.701494
-43.512231	-2.009599	1.826752	0.008220	0.701440
-43.230889	-2.058092	1.831757	0.008167	0.701444
-42.953884	-2.110205	1.836762	0.008116	0.701438
-43.214600	-2.061286	1.841766	0.008164	0.701443
-43.249826	-2.053764	1.846771	0.008171	0.701445
-43.135700	-2.102891	1.851776	0.008150	0.701387
-43.629697	-2.142579	1.856781	0.008242	0.701128
-44.017768	-2.077079	1.861786	0.008314	0.701121
-44.192656	-2.045582	1.866790	0.008346	0.701121
-43.634485	-2.142315	1.871795	0.008243	0.701127
-43.890299	-2.099933	1.876800	0.008290	0.701120
-44.249588	-2.029664	1.881805	0.008357	0.701133
-44.067265	-2.145170	1.886810	0.008323	0.700965
-44.697527	-2.075886	1.891814	0.008440	0.700877
-44.695045	-2.072622	1.896819	0.008440	0.700885
-44.863871	-2.047905	1.901824	0.008471	0.700874
-44.758803	-2.059620	1.906829	0.008452	0.700888
-45.054178	-2.011068	1.911834	0.008507	0.700880
-44.963201	-2.035059	1.916838	0.008490	0.700864
-45.392489	-2.107889	1.921843	0.008570	0.700561
-45.804807	-2.044373	1.926848	0.008647	0.700541
-45.997059	-2.001387	1.931853	0.008682	0.700559
-45.671491	-2.065738	1.936858	0.008622	0.700546
-45.632891	-2.073073	1.941862	0.008615	0.700545
-45.603012	-2.079084	1.946867	0.008609	0.700544
-45.723499	-2.092694	1.951872	0.008632	0.700472
-45.984366	-2.167074	1.956877	0.008680	0.700227
-46.294298	-2.113574	1.961882	0.008738	0.700224
-46.752653	-2.029455	1.966886	0.008823	0.700228
-46.287944	-2.111419	1.971891	0.008737	0.700230
-46.596832	-2.058643	1.976896	0.008794	0.700225
-46.504144	-2.073660	1.981901	0.008777	0.700229
-46.840714	-2.130574	1.986906	0.008840	0.699991
-47.484809	-2.059253	1.991910	0.008960	0.699903
-47.240380	-2.098905	1.996915	0.008914	0.699911
-47.462148	-2.060584	2.001920	0.008955	0.699908

-47.535832	-2.051047	2.011917	0.008969	0.699901
-47.388792	-2.077670	2.021914	0.008942	0.699900
-48.031203	-2.096066	2.031910	0.009061	0.699630
-47.978805	-2.116129	2.041907	0.009052	0.699608
-48.314598	-2.057930	2.051904	0.009114	0.699605
-48.221753	-2.073351	2.061901	0.009097	0.699607
-47.638546	-2.033588	2.071898	0.008988	0.699899
-47.513017	-2.050562	2.081894	0.008965	0.699910
-47.397740	-2.074640	2.091891	0.008944	0.699903
-47.430823	-2.070918	2.101888	0.008950	0.699898
-47.246656	-2.103930	2.111885	0.008916	0.699898
-47.277048	-2.099033	2.121882	0.008921	0.699897
-47.671773	-2.023205	2.131878	0.008995	0.699908
-47.511958	-2.050027	2.141875	0.008965	0.699911
-47.246365	-2.027360	2.151872	0.008916	0.700053
-46.373053	-2.100053	2.161869	0.008753	0.700222
-46.699543	-2.038894	2.171866	0.008814	0.700228
-46.448847	-2.084654	2.181862	0.008767	0.700225
-46.564579	-2.064348	2.191859	0.008789	0.700225
-45.866093	-2.059028	2.201856	0.008659	0.700488
-45.513480	-2.099105	2.211853	0.008593	0.700534
-45.582342	-2.086231	2.221850	0.008606	0.700535
-45.487395	-2.102718	2.231846	0.008588	0.700536
-45.063880	-2.096767	2.241843	0.008509	0.700701
-44.731828	-2.070672	2.251840	0.008448	0.700874
-44.725469	-2.071325	2.261837	0.008446	0.700875
-44.463227	-2.118063	2.271834	0.008398	0.700875
-44.444512	-2.070211	2.281830	0.008394	0.700979
-43.682322	-2.134230	2.291827	0.008252	0.701125
-44.256589	-2.030940	2.301824	0.008359	0.701126
-44.048819	-2.066152	2.311821	0.008320	0.701130
-43.359748	-2.037090	2.321818	0.008192	0.701438
-43.207392	-2.059527	2.331814	0.008164	0.701447
-42.925705	-2.110308	2.341811	0.008111	0.701446
-42.765544	-2.061576	2.351808	0.008082	0.701603
-42.111662	-2.106986	2.361805	0.007960	0.701747
-42.260431	-2.078785	2.371802	0.007988	0.701750
-42.250755	-2.077017	2.381798	0.007986	0.701757
-41.571531	-2.037786	2.391795	0.007859	0.702081
-41.481166	-2.054728	2.401792	0.007843	0.702080
-41.394246	-2.071210	2.411789	0.007826	0.702078
-41.113779	-2.018775	2.421786	0.007774	0.702285
-40.458428	-2.091267	2.431782	0.007652	0.702374
-40.521271	-2.080162	2.441779	0.007664	0.702374
-40.516220	-2.042320	2.451776	0.007663	0.702453
-39.598944	-2.085915	2.461773	0.007492	0.702695
-39.799955	-2.049908	2.471770	0.007530	0.702695
-39.615005	-2.079768	2.481766	0.007495	0.702701
-39.019389	-2.060945	2.491763	0.007384	0.702954
-38.737210	-2.083651	2.501760	0.007332	0.703010
-38.871073	-2.060157	2.511757	0.007357	0.703009
-38.760892	-2.026745	2.521754	0.007336	0.703116
-37.720051	-2.096459	2.531750	0.007142	0.703350
-37.999571	-2.046342	2.541747	0.007194	0.703351
-37.876306	-2.069575	2.551744	0.007172	0.703348
-37.362457	-2.038568	2.561741	0.007076	0.703596
-37.234488	-2.039099	2.571738	0.007052	0.703640
-36.867642	-2.103120	2.581734	0.006984	0.703643
-36.960606	-2.019580	2.591731	0.007001	0.703778
-36.216494	-2.063550	2.601728	0.006863	0.703957
-36.498743	-2.014150	2.611725	0.006915	0.703955
-36.243598	-2.040050	2.621722	0.006868	0.703995
-35.295915	-2.072534	2.631718	0.006691	0.704270
-35.231099	-2.086007	2.641715	0.006679	0.704266
-35.307072	-2.072641	2.651712	0.006693	0.704266
-35.047979	-2.030901	2.661709	0.006645	0.704443
-34.503927	-2.051796	2.671706	0.006544	0.704596
-34.411973	-2.064020	2.681702	0.006527	0.704605
-34.599955	-2.015179	2.691699	0.006562	0.704635
-34.007587	-1.984543	2.701696	0.006451	0.704910
-33.856173	-2.013181	2.711693	0.006423	0.704907
-33.960448	-1.992793	2.721690	0.006443	0.704910
-32.882182	-2.030077	2.731686	0.006242	0.705222
-32.856862	-2.030459	2.741683	0.006237	0.705230
-32.668869	-2.065966	2.751680	0.006202	0.705226
-32.953863	-1.933178	2.761677	0.006255	0.705391
-31.847152	-2.055681	2.771674	0.006049	0.705542
-31.975012	-2.031787	2.781670	0.006073	0.705544
-32.123960	-1.972178	2.791667	0.006101	0.705611
-31.380706	-1.964929	2.801664	0.005962	0.705892
-31.465621	-1.951680	2.811661	0.005978	0.705888
-31.159195	-2.008607	2.821658	0.005921	0.705883
-30.391459	-2.019651	2.831654	0.005778	0.706136
-30.420397	-2.010279	2.841651	0.005784	0.706145
-30.370014	-2.018580	2.851648	0.005774	0.706146
-30.064503	-1.986455	2.861645	0.005718	0.706320
-29.390198	-2.036949	2.871642	0.005592	0.706460
-29.509121	-2.015581	2.881638	0.005614	0.706460
-29.858979	-1.915534	2.891635	0.005679	0.706536
-28.846478	-1.971901	2.901632	0.005491	0.706785
-29.377972	-1.868409	2.911629	0.005590	0.706803
-28.939882	-1.908305	2.921626	0.005508	0.706880
-27.760648	-2.003231	2.931622	0.005289	0.707111
-27.901459	-1.974188	2.941619	0.005315	0.707119
-28.014771	-1.958413	2.951616	0.005336	0.707110
-27.504173	-1.920901	2.961613	0.005241	0.707368
-27.220441	-1.950735	2.971610	0.005188	0.707409
-27.304721	-1.933050	2.981606	0.005204	0.707415
-26.703939	-1.932581	2.991603	0.005092	0.707631
-26.055556	-2.004798	3.001600	0.004971	0.707717
-26.018923	-2.011893	3.011597	0.004965	0.707716
-26.075227	-1.997050	3.021594	0.004975	0.707726
-25.312153	-1.978221	3.031590	0.004833	0.708036
-24.981264	-2.039467	3.041587	0.004771	0.708032
-25.109508	-2.019441	3.051584	0.004795	0.708026
-24.899152	-2.037462	3.061581	0.004756	0.708065
-24.137731	-2.024924	3.071578	0.004614	0.708362
-24.113069	-2.025440	3.081574	0.004610	0.708370
-24.170742	-2.015106	3.091571	0.004621	0.708370
-24.195966	-1.939742	3.101568	0.004625	0.708512
-23.662496	-1.956625	3.111565	0.004526	0.708669
-23.470766	-1.995921	3.121562	0.004490	0.708658
-23.277922	-2.020672	3.131558	0.004454	0.708678
-22.435717	-2.022193	3.141555	0.004298	0.708975
-22.518415	-2.009937	3.151552	0.004313	0.708970
-22.563468	-2.000876	3.161549	0.004321	0.708972
-22.131056	-2.018860	3.171546	0.004241	0.709090
-21.518735	-2.033325	3.181542	0.004127	0.709280
-21.525217	-2.030005	3.191539	0.004128	0.709284
-21.787209	-1.984006	3.201536	0.004177	0.709283
-20.890247	-1.999208	3.211533	0.004010	0.709572
-20.551303	-2.041265	3.221530	0.003947	0.709609
-20.749989	-2.002641	3.231526	0.003984	0.709615
-20.657753	-1.977181	3.241523	0.003967	0.709699
-19.725393	-2.039320	3.251520	0.003793	0.709907
-19.645765	-2.054936	3.261517	0.003778	0.709904
-19.791826	-2.020999	3.271514	0.003806	0.709920
-19.505278	-1.967445	3.281510	0.003752	0.710129
-18.822183	-2.036204	3.291507	0.003625	0.710235
-19.196944	-1.966637	3.301504	0.003695	0.710240
-18.917208	-1.984634	3.311501	0.003643	0.710304
-17.875870	-2.049074	3.321498	0.003449	0.710546
-17.962682	-2.034058	3.331494	0.003465	0.710545
-17.895275	-2.043234	3.341491	0.003453	0.710550
-17.698537	-1.975613	3.351488	0.003416	0.710756
-17.074337	-2.020871	3.361485	0.003300	0.710887
-17.320966	-1.970611	3.371482	0.003346	0.710900
-16.863559	-2.054788	3.381478	0.003261	0.710894
-16.388201	-2.009350	3.391475	0.003172	0.711154
-16.311318	-2.024870	3.401472	0.003158	0.711151
-16.090622	-2.065621	3.411469	0.003117	0.711148
-16.018195	-2.015625	3.421466	0.003103	0.711273
-15.076876	-2.086620	3.431462	0.002928	0.711466
-15.330047	-2.037697	3.441459	0.002975	0.711474
-15.614821	-1.986631	3.451456	0.003028	0.711474
-14.808270	-1.992521	3.461453	0.002878	0.711749
-14.756657	-1.990060	3.471450	0.002868	0.711772
-14.482029	-2.034541	3.481446	0.002817	0.711781
-14.279864	-1.977419	3.491443	0.002780	0.711967
-13.767434	-2.001618	3.501440	0.002684	0.712101
-13.535950	-2.040252	3.511437	0.002641	0.712106
-13.777184	-1.972322	3.521434	0.002686	0.712155
-12.736198	-2.030539	3.531430	0.002492	0.712409
-12.535171	-2.066569	3.541427	0.002455	0.712409
-13.160542	-1.952829	3.551424	0.002571	0.712413
-12.539273	-1.945955	3.561421	0.002456	0.712647
-12.277857	-1.947500	3.571418	0.002407	0.712737
-11.983594	-1.998137	3.581414	0.002352	0.712740
-11.636830	-2.003497	3.591411	0.002288	0.712853
-10.965966	-2.028149	3.601408	0.002163	0.713042
-11.076027	-2.008446	3.611405	0.002183	0.713042
-11.018467	-2.023119	3.621402	0.002173	0.713033
-10.501258	-1.986716	3.631398	0.002076	0.713289
-10.486359	-1.941435	3.641395	0.002074	0.713384
-9.927179	-2.047154	3.651392	0.001969	0.713372
-10.101216	-1.980232	3.661389	0.002002	0.713443
-9.262154	-2.015072	3.671386	0.001846	0.713671
-9.057629	-2.047321	3.681382	0.001808	0.713679
-9.223974	-2.019361	3.691379	0.001839	0.713676
-8.471173	-2.071340	3.701376	0.001698	0.713839
-7.939041	-2.089180	3.711373	0.001599	0.713992
-8.144212	-2.056075	3.721370	0.001638	0.713985
-7.812997	-2.115095	3.731366	0.001576	0.713985
-7.765600	-2.066312	3.741363	0.001567	0.714099
-7.050946	-2.091302	3.751360	0.001434	0.714302
-7.319785	-2.045050	3.761357	0.001484	0.714299
-7.292303	-2.050556	3.771354	0.001479	0.714298
-6.625987	-2.065725	3.781350	0.001355	0.714503
-6.224883	-2.076911	3.791347	0.001280	0.714623
-6.070732	-2.105137	3.801344	0.001252	0.714621
-6.246473	-2.074406	3.811341	0.001284	0.714620
-5.362624	-2.113193	3.821338	0.001120	0.714856
-5.090289	-2.131606	3.831334	0.001069	0.714916
-5.058937	-2.137251	3.841331	0.001063	0.714915
-4.950057	-2.156076	3.851328	0.001043	0.714917
-4.679732	-2.077495	3.861325	0.000993	0.715168
-4.605642	-2.051131	3.871322	0.000979	0.715246
-4.540077	-2.057040	3.881318	0.000967	0.715258
-4.406842	-2.029388	3.891315	0.000942	0.715360
-3.621865	-2.060358	3.901312	0.000796	0.715576
-3.497007	-2.091090	3.911309	0.000773	0.715559
-3.341181	-2.118511	3.921306	0.000744	0.715559
-2.838762	-2.086626	3.931302	0.000650	0.715800
-2.463285	-2.105032	3.941299	0.000580	0.715896
-2.063897	-2.177211	3.951296	0.000506	0.715894
-2.207252	-2.149730	3.961293	0.000533	0.715898
-1.885369	-2.129008	3.971290	0.000473	0.716052
-1.656275	-2.125899	3.981286	0.000430	0.716139
-1.592802	-2.134031	3.991283	0.000418	0.716146
-1.471346	-2.148742	4.001280	0.000396	0.716159
-1.365572	-2.017578	4.011277	0.000376	0.716456
-0.958238	-2.091762	4.021274	0.000300	0.716453
-1.155046	-2.052748	4.031270	0.000337	0.716461
-0.952392	-1.934865	4.041267	0.000299	0.716766
-0.850701	-1.954023	4.051264	0.000280	0.716764
-0.764572	-1.906969	4.061261	0.000264	0.716887
-0.712325	-1.807943	4.071258	0.000254	0.717102
-0.626008	-1.809948	4.081254	0.000238	0.717128
-0.706936	-1.657221	4.091251	0.000253	0.717402
-1.386564	-1.487888	4.101248	0.000380	0.717497
-1.024484	-1.439716	4.111245	0.000312	0.717720
-0.501087	-1.435774	4.121242	0.000215	0.717912
-0.205726	-1.429990	4.131238	0.000160	0.718027
-0.159574	-1.295011	4.141235	0.000151	0.718310
-0.146145	-1.245478	4.151232	0.000149	0.718413
-0.052442	-1.137650	4.161229	0.000131	0.718658
-0.438007	-0.965460	4.171226	0.000203	0.718863
-0.193300	-0.912165	4.181222	0.000157	0.719054
-0.099833	-0.811710	4.191219	0.000140	0.719285
0.012754	-0.678163	4.201216	0.000119	0.719588
-0.099657	-0.546473	4.211213	0.000140	0.719808
0.419632	-0.528930	4.221210	0.000043	0.720025
0.426524	-0.403776	4.231206	0.000042	0.720274
0.388546	-0.252096	4.241203	0.000049	0.720559
0.130629	-0.045321	4.251200	0.000097	0.720876
0.000000	0.107932	4.261197	0.000121	0.721132

0.090466	0.721145	4.266202	0.000104	0.722369
0.401546	1.937450	4.271206	0.000045	0.724863
0.659625	3.748558	4.276211	-0.000004	0.728489
1.205667	6.073988	4.281216	-0.000108	0.733192
1.543239	8.937529	4.286221	-0.000172	0.738829
1.601078	12.336281	4.291226	-0.000185	0.745347
2.023270	16.124319	4.296230	-0.000266	0.752665
2.650671	20.268577	4.301235	-0.000386	0.760646
3.048015	24.869385	4.306240	-0.000463	0.769310
3.191209	29.874484	4.311245	-0.000493	0.778533
3.871237	35.130941	4.316250	-0.000623	0.788271
4.150059	40.785583	4.321254	-0.000678	0.798472
4.654503	46.685671	4.326259	-0.000776	0.809045
5.594010	52.803647	4.331264	-0.000955	0.819991
6.830378	59.149595	4.336269	-0.001189	0.831271
7.574225	65.818786	4.341274	-0.001332	0.842798
8.015681	72.767169	4.346278	-0.001419	0.854543
8.901227	79.826948	4.351283	-0.001588	0.866440
11.431306	86.832113	4.356288	-0.002064	0.878554
11.682756	94.406113	4.361293	-0.002116	0.890770
12.477172	102.037468	4.366298	-0.002269	0.903060
13.661992	109.758749	4.371302	-0.002494	0.915430
14.879256	117.580807	4.376307	-0.002726	0.927798
15.898864	125.592891	4.381312	-0.002921	0.940236
16.520091	133.760748	4.386317	-0.003042	0.952640
17.292169	141.992955	4.391322	-0.003191	0.965017
18.116828	150.308198	4.396326	-0.003350	0.977371
19.254465	158.644824	4.401331	-0.003567	0.989678
20.257651	167.068068	4.406336	-0.003760	1.001924
20.835596	175.577349	4.411341	-0.003873	1.014038
21.989026	184.028690	4.416346	-0.004093	1.026066
22.784633	192.593190	4.421350	-0.004247	1.038025
23.262677	201.224093	4.426355	-0.004341	1.049862
24.064113	209.831568	4.431360	-0.004496	1.061610
25.031885	218.443030	4.436365	-0.004682	1.073273
25.872770	227.059736	4.441370	-0.004844	1.084787
26.180282	235.790963	4.446374	-0.004907	1.096210
26.717747	244.463786	4.451379	-0.005013	1.107490
28.066429	253.017413	4.456384	-0.005270	1.118682
28.311989	261.758799	4.461389	-0.005321	1.129761
29.048455	270.408740	4.466394	-0.005464	1.140723
29.453916	279.134280	4.471398	-0.005545	1.151603
30.635419	287.669507	4.476403	-0.005771	1.162311
31.996898	296.184171	4.481408	-0.006030	1.172932
32.808776	304.792831	4.486413	-0.006186	1.183459
33.382768	313.449128	4.491418	-0.006299	1.193900
34.125772	322.034100	4.496422	-0.006443	1.204200
34.591090	330.659367	4.501427	-0.006535	1.214405
35.432309	339.212411	4.506432	-0.006697	1.224514
36.148190	347.798794	4.511437	-0.006836	1.234554
36.734067	356.357459	4.516442	-0.006951	1.244457
37.675338	364.857943	4.521446	-0.007132	1.254283
38.130707	373.410279	4.526451	-0.007222	1.263998
38.685500	381.957658	4.531456	-0.007331	1.273652
39.218171	390.457609	4.536461	-0.007436	1.283176
39.896871	398.943353	4.541466	-0.007567	1.292642
40.704570	407.393216	4.546470	-0.007723	1.302023
40.979314	415.993694	4.551475	-0.007780	1.311402
41.695230	424.467035	4.556480	-0.007919	1.320658
42.072562	432.903938	4.561485	-0.007995	1.329750
42.830875	441.281538	4.566490	-0.008141	1.338784
43.443368	449.686248	4.571494	-0.008261	1.347761
44.199818	458.061689	4.576499	-0.008407	1.356672
44.699814	466.457531	4.581504	-0.008506	1.365502
45.315144	474.844915	4.586509	-0.008626	1.374285
45.813235	483.228335	4.591514	-0.008724	1.382989
46.484811	491.605218	4.596518	-0.008854	1.391661
46.662577	500.020723	4.601523	-0.008893	1.400235
47.547751	508.302063	4.606528	-0.009063	1.408739
47.963548	516.665408	4.611533	-0.009146	1.417197
48.723897	524.929097	4.616538	-0.009293	1.425561
49.294557	533.279757	4.621542	-0.009405	1.433932
49.989245	541.555942	4.626547	-0.009539	1.442201
50.051862	549.977114	4.631552	-0.009557	1.450462
50.484775	558.287323	4.636557	-0.009643	1.458628
51.100043	566.573010	4.641562	-0.009763	1.466753
52.042288	574.859607	4.646566	-0.009943	1.474886
52.621918	583.122258	4.651571	-0.010057	1.482894
53.353813	591.370708	4.656576	-0.010198	1.490869
53.886845	599.651407	4.661581	-0.010303	1.498801
54.199804	607.958509	4.666586	-0.010367	1.506682
54.908955	616.214535	4.671590	-0.010504	1.514535
55.013251	624.536442	4.676595	-0.010529	1.522316
55.672680	632.755340	4.681600	-0.010657	1.530046
56.045959	641.030245	4.686605	-0.010732	1.537746
56.567865	649.270974	4.691610	-0.010834	1.545398
56.790678	657.589505	4.696614	-0.010881	1.553039
57.399960	665.786985	4.701619	-0.011000	1.560589
57.887361	674.029256	4.706624	-0.011096	1.568126
58.386399	682.256131	4.711629	-0.011194	1.575614
58.923257	690.465250	4.716634	-0.011300	1.583056
59.481735	698.691460	4.721638	-0.011409	1.590481
59.804873	706.950608	4.726643	-0.011475	1.597867
60.270649	715.160614	4.731648	-0.011567	1.605196
60.705813	723.385210	4.736653	-0.011653	1.612500
61.206616	731.581283	4.741658	-0.011752	1.619755
61.443562	739.831792	4.746662	-0.011801	1.626988
61.905153	748.066917	4.751667	-0.011892	1.634207
62.724716	756.185926	4.756672	-0.012050	1.641343
63.195642	764.372747	4.761677	-0.012143	1.648458
63.461208	772.607729	4.766682	-0.012198	1.655556
64.031544	780.775948	4.771686	-0.012310	1.662608
64.124132	789.031548	4.776691	-0.012332	1.669640
64.616200	797.214851	4.781696	-0.012429	1.676634
64.923991	805.378752	4.786701	-0.012492	1.683559
65.523630	813.531827	4.791706	-0.012609	1.690484
65.718855	821.766557	4.796710	-0.012651	1.697396
66.405874	829.875900	4.801715	-0.012784	1.704240
67.431372	837.986631	4.806720	-0.012980	1.711102
68.087572	846.149320	4.811725	-0.013107	1.717931
68.378477	854.349334	4.816730	-0.013167	1.724716
68.864847	862.538166	4.821734	-0.013263	1.731490
69.527105	870.672869	4.826739	-0.013391	1.738217
69.660531	878.902879	4.831744	-0.013422	1.744927
70.051164	887.084610	4.836749	-0.013500	1.751605
70.213243	895.298186	4.841754	-0.013535	1.758254
70.708722	903.437040	4.846758	-0.013633	1.764860
71.125687	911.591797	4.851763	-0.013716	1.771444
72.029956	919.684374	4.856768	-0.013889	1.778015
72.279363	927.863801	4.861773	-0.013941	1.784549
72.665739	936.047321	4.866778	-0.014018	1.791079
73.312414	944.201213	4.871782	-0.014144	1.797594
73.462575	952.365658	4.876787	-0.014177	1.804033
74.011221	960.482763	4.881792	-0.014285	1.810460
74.461346	968.611414	4.886797	-0.014374	1.816862
74.933508	976.739071	4.891802	-0.014467	1.823243
75.541493	984.871158	4.896806	-0.014586	1.829621
75.758633	993.045708	4.901811	-0.014631	1.835963
76.305868	1001.167257	4.906816	-0.014739	1.842281
76.780172	1009.298648	4.911821	-0.014832	1.848577
77.320380	1017.434854	4.916826	-0.014938	1.854862
78.005272	1025.547742	4.921830	-0.015071	1.861125
78.737249	1033.639848	4.926835	-0.015212	1.867356
79.150741	1041.832588	4.931840	-0.015295	1.873606
79.067259	1050.041689	4.936845	-0.015285	1.879791
79.436676	1058.138045	4.941850	-0.015359	1.885922
79.875039	1066.270456	4.946854	-0.015445	1.892068
80.035973	1074.440606	4.951859	-0.015481	1.898191
80.788933	1082.503380	4.956864	-0.015626	1.904280
80.791206	1090.708474	4.961869	-0.015632	1.910372
81.324469	1098.789254	4.966874	-0.015737	1.916411
82.059728	1106.843727	4.971878	-0.015879	1.922435
82.524285	1114.956817	4.976883	-0.015970	1.928452
83.021564	1123.101420	4.981888	-0.016068	1.934478
82.960905	1131.305613	4.986893	-0.016062	1.940466
83.439868	1139.385726	4.991898	-0.016157	1.946405
84.415051	1147.477751	4.996902	-0.016344	1.952389
84.495291	1155.661981	5.001907	-0.016364	1.958323
85.027507	1163.705066	5.006912	-0.016468	1.964187
84.997028	1171.873773	5.011917	-0.016468	1.970063
85.567612	1179.943101	5.016922	-0.016579	1.975914
85.876786	1188.074876	5.021926	-0.016642	1.981765
86.256661	1196.156685	5.026931	-0.016718	1.987570
86.633331	1204.287993	5.031936	-0.016794	1.993394
87.077590	1212.367487	5.036941	-0.016882	1.999170
87.597675	1220.433207	5.041946	-0.016984	2.004928
88.072282	1228.554783	5.046950	-0.017077	2.010704
88.430924	1236.673662	5.051955	-0.017149	2.016449
88.806847	1244.788267	5.056960	-0.017225	2.022177
89.399405	1252.874189	5.061965	-0.017340	2.027890
89.677564	1261.027399	5.066970	-0.017397	2.033602
90.165399	1269.121273	5.071974	-0.017494	2.039278
90.542947	1277.188887	5.076979	-0.017569	2.044909
90.934321	1285.314119	5.081984	-0.017647	2.050566
91.343310	1293.406940	5.086989	-0.017729	2.056186
91.617407	1301.498747	5.091994	-0.017785	2.061777
92.156259	1309.584633	5.096998	-0.017891	2.067374
92.089459	1317.758218	5.102003	-0.017883	2.072956
92.422750	1325.863299	5.107008	-0.017951	2.078517
92.999097	1333.895308	5.112013	-0.018063	2.084036
93.279443	1342.005605	5.117018	-0.018121	2.089565
93.398443	1350.173003	5.122022	-0.018148	2.095102
93.960111	1358.203575	5.127027	-0.018258	2.100575
94.742056	1366.243007	5.132032	-0.018409	2.106061
94.940494	1374.411010	5.137037	-0.018451	2.111563
95.346330	1382.526953	5.142042	-0.018532	2.117035
95.833375	1390.577168	5.147046	-0.018628	2.122457
96.033423	1398.672685	5.152051	-0.018670	2.127867
96.471151	1406.780529	5.157056	-0.018757	2.133295
97.029188	1414.826565	5.162061	-0.018866	2.138680
97.435486	1422.887355	5.167066	-0.018947	2.144046
97.798517	1430.996653	5.172070	-0.019020	2.149426
98.214207	1439.077934	5.177075	-0.019103	2.154780
98.315038	1447.206385	5.182080	-0.019127	2.160121
98.375626	1455.316587	5.187085	-0.019143	2.165434
98.917911	1463.336678	5.192090	-0.019250	2.170719
99.254085	1471.458537	5.197094	-0.019317	2.176039
99.846391	1479.485576	5.202099	-0.019433	2.181308
100.164715	1487.579917	5.207104	-0.019498	2.186582
100.522737	1495.701983	5.212109	-0.019569	2.191865
100.501535	1503.836104	5.217114	-0.019571	2.197109
100.748870	1511.913203	5.222118	-0.019622	2.202328
100.793879	1520.000131	5.227123	-0.019636	2.207522
101.319135	1528.063344	5.232128	-0.019739	2.212732
101.903006	1536.093943	5.237133	-0.019853	2.217914
102.105963	1544.181670	5.242138	-0.019896	2.223087
102.501809	1552.275669	5.247142	-0.019975	2.228268
102.916424	1560.353419	5.252147	-0.020057	2.233429
103.173956	1568.430342	5.257152	-0.020110	2.238563
103.620056	1576.475980	5.262157	-0.020199	2.243682
104.130021	1584.531196	5.267162	-0.020299	2.248802
104.367999	1592.671018	5.272166	-0.020349	2.253938
104.603548	1600.733983	5.277171	-0.020398	2.259015
104.808267	1608.838268	5.282176	-0.020441	2.264103
105.179681	1616.903095	5.287181	-0.020515	2.269170
105.337805	1625.075139	5.292186	-0.020550	2.274274
105.825802	1633.087407	5.297190	-0.020646	2.279295
106.246237	1641.105833	5.302195	-0.020730	2.284303
106.236249	1649.221046	5.307200	-0.020733	2.289324
106.641988	1657.286366	5.312205	-0.020814	2.294337
107.010772	1665.321926	5.317210	-0.020888	2.299319
107.542908	1673.359934	5.322214	-0.020992	2.304304
107.821015	1681.449442	5.327219	-0.021049	2.309289
108.243584	1689.535637	5.332224	-0.021133	2.314274
108.909749	1697.549813	5.337229	-0.021262	2.319223
109.112767	1705.627443	5.342234	-0.021305	2.324163
109.646946	1713.691787	5.347238	-0.021410	2.329111
109.790832	1721.805770	5.352243	-0.021442	2.334046
110.124739	1729.873350	5.357248	-0.021510	2.338959
110.320434	1737.966232	5.362253	-0.021551	2.343865
110.674078	1746.018071	5.367258	-0.021622	2.348749
110.953769	1754.156370	5.372262	-0.021680	2.353668
111.113137	1762.220112	5.377267	-0.021715	2.358523
111.683370	1770.202544	5.382272	-0.021826	2.363353
111.961857	1778.279041	5.387277	-0.021883	2.368205
112.346501	1786.345491	5.392282	-0.021960	2.373049
112.621749	1794.439675	5.397286	-0.022017	2.377892
113.009641	1802.463448	5.402291	-0.022094	2.382691
113.492472	1810.506798	5.407296	-0.022189	2.387500
113.717735	1818.625066	5.412301	-0.022236	2.392323
113.989279	1826.697640	5.417306	-0.022292	2.397113
114.391537	1834.742934	5.422310	-0.022372	2.401888
114.688900	1842.787632	5.427315	-0.022433	2.406645
114.940768	1850.896260	5.432320	-0.022485	2.411426
115.378558	1858.961888	5.437325	-0.022572	2.416186
115.906267	1866.964248	5.442330	-0.022675	2.420908
116.468107	1875.012879	5.447334	-0.022785	2.425649
116.629961	1883.100035	5.452339	-0.022821	2.430373
117.011941	1891.248250	5.457344	-0.022897	2.435140
117.156271	1899.293400	5.462349	-0.022929	2.439820
117.485455	1907.305303	5.467354	-0.022996	2.444485
117.728242	1915.397837	5.472358	-0.023046	2.449182
117.867589	1923.470586	5.477363	-0.023077	2.453850
118.194933	1931.517708	5.482368	-0.023144	2.458509
118.611114	1939.546712	5.487373	-0.023226	2.463155
118.632043	1947.646152	5.492378	-0.023235	2.467803
118.850181	1955.745347	5.497382	-0.023281	2.472457
119.275334	1963.759543	5.502387	-0.023366	2.477069
119.580259	1971.804812	5.507392	-0.023428	2.481681
119.942319	1979.858681	5.512397	-0.023500	2.486294
120.067118	1987.937508	5.517402	-0.023529	2.490895
120.437021	1996.018194	5.522406	-0.023603	2.495506
120.515772	2004.068519	5.527411	-0.023623	2.500070
120.839685	2012.119224	5.532416	-0.023688	2.504644
121.432035	2020.140971	5.537421	-0.023804	2.509213
121.792534	2028.236581	5.542426	-0.023876	2.513798
122.143230	2036.296207	5.547430	-0.023947	2.518353
122.595350	2044.266636	5.552435	-0.024036	2.522858
122.928775	2052.331747	5.557440	-0.024104	2.527399
123.329708	2060.387049	5.562445	-0.024183	2.531931
123.526699	2068.480192	5.567450	-0.024225	2.536461
124.151585	2076.487865	5.572454	-0.024347	2.540966
124.203092	2084.570788	5.577459	-0.024362	2.545465
124.468665	2092.646572	5.582464	-0.024417	2.549966
125.130179	2100.676024	5.587469	-0.024545	2.554462
125.399121	2108.706326	5.592474	-0.024600	2.558922
125.576800	2116.796555	5.597478	-0.024639	2.563402
125.772982	2124.855074	5.602483	-0.024680	2.567857
126.150489	2132.908058	5.607488	-0.024756	2.572314
126.240119	2141.019615	5.612493	-0.024778	2.576776
126.620607	2149.014266	5.617498	-0.024854	2.581186
127.045851	2157.070035	5.622502	-0.024938	2.585624
127.140341	2165.159199	5.627507	-0.024961	2.590051
127.205522	2173.463543	5.632512	-0.024979	2.594586
127.586432	2181.401465	5.637517	-0.025055	2.598934
127.871471	2189.368568	5.642522	-0.025113	2.603285
128.271148	2197.389648	5.647526	-0.025193	2.607665
128.336951	2205.434105	5.652531	-0.025210	2.612028
128.503132	2213.497265	5.657536	-0.025246	2.616400
128.585433	2221.543586	5.662541	-0.025267	2.620751
129.007816	2229.522286	5.667546	-0.025351	2.625080
129.362871	2237.578729	5.672550	-0.025422	2.629440
129.708520	2245.643233	5.677555	-0.025492	2.633796
129.943011	2253.680770	5.682560	-0.025541	2.638123
130.434917	2261.706538	5.687565	-0.025637	2.642453
130.725585	2269.723338	5.692570	-0.025697	2.646758
130.942840	2277.839020	5.697574	-0.025742	2.651104
130.828610	2285.957557	5.702579	-0.025726	2.655423
131.519369	2293.898489	5.707584	-0.025860	2.659693
131.799817	2301.953630	5.712589	-0.025918	2.663990
132.313839	2309.974172	5.717594	-0.026019	2.668276
132.460940	2318.121999	5.722598	-0.026051	2.672600
132.643806	2326.171213	5.727603	-0.026091	2.676866
132.880998	2334.200776	5.732608	-0.026140	2.681119
133.315450	2342.204044	5.737613	-0.026226	2.685364
133.165070	2350.295360	5.742618	-0.026203	2.689611
133.495669	2358.344581	5.747622	-0.026270	2.693860
133.568938	2366.422678	5.752627	-0.026289	2.698101
134.583646	2374.324429	5.757632	-0.026483	2.702302
134.623824	2382.463149	5.762637	-0.026496	2.706559
134.480597	2390.558185	5.767642	-0.026475	2.710775
135.500567	2398.494784	5.772646	-0.026670	2.714974
135.475194	2406.566810	5.777651	-0.026670	2.719173
135.829446	2414.594798	5.782656	-0.026741	2.723365
136.359916	2422.627729	5.787661	-0.026845	2.727565
136.649761	2430.666242	5.792666	-0.026905	2.731746
137.081333	2438.762732	5.797670	-0.026990	2.735959
137.121702	2446.820680	5.802675	-0.027003	2.740122
137.418118	2454.841971	5.807680	-0.027063	2.744275
137.686801	2462.927411	5.812685	-0.027119	2.748453
137.817295	2471.044576	5.817690	-0.027148	2.752633
138.028753	2479.132407	5.822694	-0.027193	2.756796
138.332480	2487.089485	5.827699	-0.027255	2.760892
138.516349	2495.106751	5.832704	-0.027294	2.765004
138.678285	2503.177764	5.837709	-0.027329	2.769137
138.968939	2511.213492	5.842714	-0.027389	2.773254
139.451903	2519.234080	5.847718	-0.027484	2.777368
139.538819	2527.271622	5.852723	-0.027505	2.781461
140.000087	2535.270944	5.857728	-0.027596	2.785550
140.170407	2543.360284	5.862733	-0.027633	2.789662
140.407183	2551.415121	5.867738	-0.027683	2.793754
140.586711	2559.445250	5.872742	-0.027721	2.797825
140.694326	2567.515873	5.877747	-0.027747	2.801906
141.176491	2575.495213	5.882752	-0.027842	2.805956
141.701969	2583.524841	5.887757	-0.027945	2.810028
141.598882	2591.640826	5.892762	-0.027931	2.814102
141.867828	2599.696149	5.897766	-0.027986	2.818161
142.535344	2607.646110	5.902771	-0.028116	2.822183
143.106347	2615.655610	5.907776	-0.028227	2.826224
143.470549	2623.733531	5.912781	-0.028300	2.830282
143.509261	2631.842021	5.917786	-0.028313	2.834331
143.538435	2639.936256	5.922790	-0.028323	2.838366
143.536250	2647.977772	5.927795	-0.028328	2.842367
143.627014	2656.016366	5.932800	-0.028350	2.846367
143.802109	2664.077602	5.937805	-0.028388	2.850377
144.548183	2671.993406	5.942810	-0.028532	2.854341
145.087358	2680.035405	5.947814	-0.028638	2.858350
145.418791	2688.048420	5.952819	-0.028705	2.862328
145.711320	2696.102450	5.957824	-0.028764	2.866318
146.096856	2704.159388	5.962829	-0.028842	2.870309
145.998315	2712.267748	5.967834	-0.028828	2.874294
146.405048	2720.290402	5.972838	-0.028909	2.878258
146.654802	2728.297214	5.977843	-0.028961	2.882200
146.943932	2736.308216	5.982848	-0.029020	2.886142
147.529390	2744.300730	5.987853	-0.029134	2.890084
147.606987	2752.437311	5.992858	-0.029154	2.894065
147.998291	2760.466682	5.997862	-0.029232	2.898004
147.873294	2768.514031	6.002867	-0.029214	2.901919
148.231531	2776.548615	6.007872	-0.029286	2.905848
148.470808	2784.607325	6.012877	-0.029336	2.909778
148.461843	2792.778270	6.017882	-0.029340	2.913743
148.414677	2800.842058	6.022886	-0.029336	2.917649
148.881917	2808.755310	6.027891	-0.029428	2.921504
149.162066	2816.723557	6.032896	-0.029485	2.925370
149.638858	2824.748430	6.037901	-0.029579	2.929270
149.742496	2832.821510	6.042906	-0.029604	2.933167
149.843778	2840.890075	6.047910	-0.029628	2.937057
149.962287	2848.928552	6.052915	-0.029655	2.940928
150.419136	2856.880022	6.057920	-0.029746	2.944770
150.570268	2864.961703	6.062925	-0.029779	2.948654
150.682170	2873.027687	6.067930	-0.029805	2.952523
151.265956	2881.052364	6.072934	-0.029919	2.956391
151.446039	2889.047406	6.077939	-0.029958	2.960219
151.604839	2897.101017	6.082944	-0.029993	2.964069
151.554104	2905.215098	6.087949	-0.029988	2.967932
151.737811	2913.230055	6.092954	-0.030028	2.971755
152.048997	2921.275408	6.097958	-0.030091	2.975594
152.028681	2929.309902	6.102963	-0.030092	2.979406
152.382919	2937.300495	6.107968	-0.030164	2.983211
152.598977	2945.368896	6.112973	-0.030209	2.987041
153.068875	2953.323839	6.117978	-0.030302	2.990825
153.113715	2961.474169	6.122982	-0.030315	2.994676
153.741344	2969.439240	6.127987	-0.030437	2.998463
153.780465	2977.494405	6.132992	-0.030450	3.002258
154.162055	2985.507304	6.137997	-0.030526	3.006046
154.173494	2993.555926	6.143002	-0.030534	3.009827
154.773333	3001.597879	6.148006	-0.030651	3.013629
154.666942	3009.688553	6.153011	-0.030636	3.017415
155.183270	3017.649151	6.158016	-0.030737	3.021165
155.840101	3025.616697	6.163021	-0.030865	3.024921
156.010040	3033.669027	6.168026	-0.030902	3.028688
156.230773	3041.760400	6.173030	-0.030948	3.032471
156.790520	3049.782064	6.178035	-0.031058	3.036233
156.860179	3057.817433	6.183040	-0.031076	3.039973
157.135949	3065.842898	6.188045	-0.031132	3.043714
157.341603	3073.867399	6.193050	-0.031176	3.047446
157.962737	3081.925377	6.198054	-0.031297	3.051209
158.240788	3089.965245	6.203059	-0.031354	3.054943
158.316027	3098.004698	6.208064	-0.031373	3.058662
158.620899	3106.065115	6.213069	-0.031435	3.062397
158.992748	3114.061654	6.218074	-0.031509	3.066102
159.271934	3122.121555	6.223078	-0.031567	3.069826
159.453782	3130.244720	6.228083	-0.031606	3.073571
159.753188	3138.238848	6.233088	-0.031667	3.077257
159.916025	3146.284408	6.238093	-0.031702	3.080956
159.928289	3154.269672	6.243098	-0.031710	3.084616
160.265290	3162.319857	6.248102	-0.031778	3.088316
160.521919	3170.323702	6.253107	-0.031831	3.091987
160.904760	3178.338253	6.258112	-0.031907	3.095664
161.254075	3186.373419	6.263117	-0.031977	3.099344
161.274878	3194.426372	6.268122	-0.031987	3.103014
161.522749	3202.466291	6.273126	-0.032038	3.106683
161.628904	3210.508607	6.278131	-0.032063	3.110343
161.634411	3218.586944	6.283136	-0.032069	3.114010
162.020806	3226.604083	6.288141	-0.032146	3.117662
162.147010	3234.610972	6.293146	-0.032175	3.121293
162.824040	3242.581991	6.298150	-0.032306	3.124929
162.699726	3250.666292	6.303155	-0.032288	3.128576
162.880205	3258.694078	6.308160	-0.032327	3.132206
163.411954	3266.743327	6.313165	-0.032432	3.135858
163.612703	3274.728409	6.318170	-0.032474	3.139462
163.779809	3282.796910	6.323174	-0.032510	3.143097
163.807729	3290.859872	6.328179	-0.032521	3.146720
164.236076	3298.841046	6.333184	-0.032606	3.150319
164.445867	3306.952432	6.338189	-0.032650	3.153963
164.521695	3314.935523	6.343194	-0.032670	3.157540
164.697100	3323.001942	6.348198	-0.032707	3.161154
164.903744	3330.960663	6.353203	-0.032751	3.164717
165.139098	3338.995031	6.358208	-0.032800	3.168311
165.464872	3347.056616	6.363213	-0.032866	3.171917
165.547798	3355.122716	6.368218	-0.032887	3.175510
165.767774	3363.130805	6.373222	-0.032933	3.179080
165.906036	3371.165648	6.378227	-0.032964	3.182653
166.492265	3379.143742	6.383232	-0.033078	3.186217
166.774721	3387.205030	6.388237	-0.033136	3.189800
166.863302	3395.257195	6.393242	-0.033158	3.193368
167.352908	3403.281208	6.398246	-0.033254	3.196935
167.413934	3411.313131	6.403251	-0.033271	3.200484
167.722468	3419.311583	6.408256	-0.033333	3.204025
167.937048	3427.383172	6.413261	-0.033379	3.207590
168.219425	3435.418460	6.418266	-0.033436	3.211138
168.613127	3443.455210	6.423270	-0.033515	3.214687
168.815523	3451.478355	6.428275	-0.033558	3.218218
169.060420	3459.477261	6.433280	-0.033609	3.221737
169.338105	3467.498389	6.438285	-0.033666	3.225262
169.441461	3475.569592	6.443290	-0.033690	3.228799
169.727588	3483.644930	6.448294	-0.033749	3.232341
169.990983	3491.714208	6.453299	-0.033803	3.235875
170.262617	3499.656344	6.458304	-0.033859	3.239351
170.679382	3507.705631	6.463309	-0.033942	3.242875
170.828302	3515.711683	6.468314	-0.033974	3.246365
170.953363	3523.730772	6.473318	-0.034003	3.249857
171.005099	3531.771009	6.478323	-0.034018	3.253351
171.398367	3539.796695	6.483328	-0.034096	3.256849
171.663225	3547.811181	6.488333	-0.034151	3.260333
171.504535	3555.862735	6.493338	-0.034126	3.263812
171.886921	3563.880285	6.498342	-0.034203	3.267294
172.215833	3571.891171	6.503347	-0.034269	3.270768
172.573395	3579.924082	6.508352	-0.034341	3.274248
172.888832	3587.963716	6.513357	-0.034405	3.277726
173.016573	3595.980309	6.518362	-0.034434	3.281183
173.279412	3603.980246	6.523366	-0.034488	3.284635
173.402951	3612.048440	6.528371	-0.034517	3.288106
173.917209	3620.053979	6.533376	-0.034617	3.291562
174.125650	3628.112902	6.538381	-0.034662	3.295026
174.168394	3636.136064	6.543386	-0.034675	3.298464
174.526471	3644.182744	6.548390	-0.034747	3.301921
174.738846	3652.188077	6.553395	-0.034791	3.305351
174.756089	3660.236612	6.558400	-0.034800	3.308788
175.213902	3668.286960	6.563405	-0.034890	3.312239
175.430375	3676.326818	6.568410	-0.034936	3.315673
175.605488	3684.315639	6.573414	-0.034974	3.319080
175.677553	3692.363643	6.578419	-0.034992	3.322505
176.100663	3700.325384	6.583424	-0.035076	3.325903
176.603740	3708.373903	6.588429	-0.035175	3.329336
176.516880	3716.453493	6.593434	-0.035164	3.332758
176.389101	3724.577355	6.598438	-0.035146	3.336194
176.740314	3732.511574	6.603443	-0.035216	3.339563
177.075485	3740.485669	6.608448	-0.035284	3.342945
177.024025	3748.615975	6.613453	-0.035280	3.346375
177.331127	3756.563087	6.618458	-0.035342	3.349738
178.167587	3764.534512	6.623462	-0.035503	3.353127
178.170822	3772.651700	6.628467	-0.035509	3.356543
178.262699	3780.652967	6.633472	-0.035531	3.359911
178.477072	3788.674941	6.638477	-0.035576	3.363288
178.859817	3796.664736	6.643482	-0.035653	3.366654
179.189346	3804.697777	6.648486	-0.035719	3.370033
179.355619	3812.772237	6.653491	-0.035755	3.373420
179.518988	3820.815570	6.658496	-0.035791	3.376790
179.603388	3828.860961	6.663501	-0.035812	3.380155
179.798834	3836.871429	6.668506	-0.035854	3.383507
179.943502	3844.902429	6.673510	-0.035886	3.386861
180.264216	3852.935008	6.678515	-0.035951	3.390219
180.186320	3861.043448	6.683520	-0.035942	3.393592
180.772780	3869.004036	6.688525	-0.036056	3.396922
180.822906	3876.995400	6.693530	-0.036070	3.400244
181.233845	3884.991096	6.698534	-0.036152	3.403576
181.535014	3893.024232	6.703539	-0.036213	3.406917
181.505760	3901.063957	6.708544	-0.036213	3.410246
181.961902	3909.079202	6.713549	-0.036303	3.413578
181.911323	3917.148566	6.718554	-0.036299	3.416912
182.201045	3925.154858	6.723558	-0.036358	3.420228
182.275275	3933.190427	6.728563	-0.036377	3.423546
182.494298	3941.194012	6.733568	-0.036423	3.426852
182.852810	3949.239627	6.738573	-0.036495	3.430177
182.906650	3957.277653	6.743578	-0.036511	3.433486
182.972494	3965.355176	6.748582	-0.036528	3.436807
183.155489	3973.341341	6.753587	-0.036567	3.440092
183.402283	3981.299644	6.758592	-0.036619	3.443365
183.709943	3989.330884	6.763597	-0.036681	3.446666
183.833420	3997.375553	6.768602	-0.036709	3.449963
184.228526	4005.411655	6.773606	-0.036788	3.453263
184.601613	4013.443629	6.778611	-0.036863	3.456557
184.696732	4021.484094	6.783616	-0.036886	3.459842
185.256779	4029.476280	6.788621	-0.036995	3.463120
185.275082	4037.517576	6.793626	-0.037004	3.466397
185.484252	4045.555291	6.798630	-0.037048	3.469675
185.815927	4053.630255	6.803635	-0.037115	3.472969
186.057694	4061.662437	6.808640	-0.037165	3.476240
186.307330	4069.624735	6.813645	-0.037217	3.479480
186.567389	4077.655384	6.818650	-0.037271	3.482745
186.868870	4085.648068	6.823654	-0.037332	3.485992
187.204758	4093.690441	6.828659	-0.037400	3.489258
187.053976	4101.761976	6.833664	-0.037377	3.492517
187.371990	4109.783903	6.838669	-0.037441	3.495768
187.353112	4117.823154	6.843674	-0.037443	3.499012
187.459228	4125.816882	6.848678	-0.037468	3.502238
187.966627	4133.805885	6.853683	-0.037568	3.505472
188.033109	4141.850964	6.858688	-0.037585	3.508712
188.507304	4149.887962	6.863693	-0.037679	3.511959
188.559127	4157.940646	6.868698	-0.037694	3.515195
188.826425	4165.935409	6.873702	-0.037749	3.518412
188.769041	4174.025280	6.878707	-0.037743	3.521654
188.823056	4181.945777	6.883712	-0.037758	3.524829
189.350584	4189.992310	6.888717	-0.037862	3.528066
189.914922	4197.985921	6.893722	-0.037972	3.531279
189.908960	4206.096240	6.898726	-0.037976	3.534519
190.403285	4214.092911	6.903731	-0.038074	3.537726
190.545034	4222.104537	6.908736	-0.038105	3.540925
190.776896	4230.126194	6.913741	-0.038154	3.544128
190.947027	4238.157440	6.918746	-0.038191	3.547330
191.374218	4246.191954	6.923750	-0.038275	3.550538
191.590440	4254.359542	6.928755	-0.038321	3.553789
191.967170	4262.319920	6.933760	-0.038396	3.556960
192.424994	4270.273761	6.938765	-0.038487	3.560128
192.518590	4278.289119	6.943770	-0.038509	3.563307
192.505951	4286.353355	6.948774	-0.038512	3.566499
192.969452	4294.335708	6.953779	-0.038604	3.569670
193.259954	4302.351360	6.958784	-0.038663	3.572846
193.550621	4310.420945	6.963789	-0.038722	3.576040
193.417193	4318.414458	6.968794	-0.038703	3.579190
193.647651	4326.433162	6.973798	-0.038751	3.582357
194.060090	4334.453158	6.978803	-0.038833	3.585526
194.076257	4342.487360	6.983808	-0.038841	3.588688
194.097550	4350.579944	6.988813	-0.038850	3.591869
194.446318	4358.546672	6.993818	-0.038920	3.595008
194.682941	4366.566691	6.998822	-0.038970	3.598161
195.157737	4374.577806	7.003827	-0.039063	3.601315
195.273481	4382.541759	7.008832	-0.039090	3.604438
195.514752	4390.599618	7.013837	-0.039140	3.607598
195.707598	4398.619329	7.018842	-0.039181	3.610739
196.020187	4406.679315	7.023846	-0.039245	3.613896
196.236691	4414.725196	7.028851	-0.039290	3.617043
196.440195	4422.667766	7.033856	-0.039333	3.620146
196.884211	4430.719200	7.038861	-0.039421	3.623295
197.030414	4438.771974	7.043866	-0.039454	3.626434
197.010225	4446.803929	7.048870	-0.039455	3.629557
197.330017	4454.882908	7.053875	-0.039520	3.632706
197.609336	4462.893797	7.058880	-0.039577	3.635823
197.752729	4470.873491	7.063885	-0.039609	3.638923
197.848531	4478.864917	7.068890	-0.039632	3.642023
198.171897	4486.873535	7.073894	-0.039698	3.645133
198.338596	4494.927212	7.078899	-0.039734	3.648254
198.390603	4502.983503	7.083904	-0.039749	3.651370
198.584911	4511.046009	7.088909	-0.039790	3.654490
198.755774	4519.051525	7.093914	-0.039827	3.657584
199.073001	4527.066245	7.098918	-0.039892	3.660683
199.266673	4535.101026	7.103923	-0.039933	3.663783
199.386497	4543.115174	7.108928	-0.039960	3.666872
199.749749	4551.116722	7.113933	-0.040033	3.669959
199.795821	4559.165688	7.118938	-0.040047	3.673053
200.158285	4567.182684	7.123942	-0.040120	3.676141
200.455705	4575.179123	7.128947	-0.040180	3.679216
200.573773	4583.178685	7.133952	-0.040207	3.682286
200.862545	4591.209689	7.138957	-0.040266	3.685369
201.111728	4599.215045	7.143962	-0.040318	3.688439
201.225133	4607.293199	7.148966	-0.040344	3.691531
201.380718	4615.314952	7.153971	-0.040379	3.694600
201.154458	4623.368141	7.158976	-0.040342	3.697668
201.500487	4631.383664	7.163981	-0.040411	3.700734
201.566336	4639.328936	7.168986	-0.040429	3.703764
202.110929	4647.350141	7.173990	-0.040535	3.706831
202.159233	4655.423897	7.178995	-0.040550	3.709904
202.251337	4663.502408	7.184000	-0.040572	3.712978
202.728274	4671.553366	7.189005	-0.040666	3.716047
202.756574	4679.515324	7.194010	-0.040677	3.719069
202.917464	4687.529774	7.199014	-0.040712	3.722112
203.002704	4695.518524	7.204019	-0.040733	3.725141
203.365915	4703.498044	7.209024	-0.040806	3.728171
203.658979	4711.556310	7.214029	-0.040865	3.731226
203.636143	4719.607120	7.219034	-0.040866	3.734269
204.065502	4727.609945	7.224038	-0.040952	3.737301
204.456124	4735.643385	7.229043	-0.041030	3.740342
204.599956	4743.605995	7.234048	-0.041062	3.743347
204.940859	4751.656633	7.239053	-0.041130	3.746388
205.171051	4759.650233	7.244058	-0.041178	3.749402
205.306552	4767.710138	7.249062	-0.041209	3.752437
205.386754	4775.802442	7.254067	-0.041229	3.755480
205.531768	4783.779309	7.259072	-0.041261	3.758479
205.956860	4791.807263	7.264077	-0.041346	3.761500
206.093996	4799.774265	7.269082	-0.041376	3.764490
206.188913	4807.842755	7.274086	-0.041399	3.767515
206.565009	4815.883401	7.279091	-0.041474	3.770533
206.615552	4823.920048	7.284096	-0.041489	3.773540
206.843149	4831.970143	7.289101	-0.041537	3.776553
207.121176	4839.930937	7.294106	-0.041594	3.779532
207.351434	4847.957889	7.299110	-0.041642	3.782532
207.475792	4856.009294	7.304115	-0.041670	3.785536
207.619669	4863.970428	7.309120	-0.041702	3.788505
207.861266	4872.036202	7.314125	-0.041752	3.791512
208.319864	4880.090790	7.319130	-0.041843	3.794518
208.470613	4888.083314	7.324134	-0.041876	3.797491
208.688662	4896.080798	7.329139	-0.041922	3.800465
208.838293	4904.063348	7.334144	-0.041955	3.803430
209.174176	4912.114767	7.339149	-0.042023	3.806422
209.308551	4920.099930	7.344154	-0.042053	3.809383
209.712222	4928.158658	7.349158	-0.042133	3.812375
209.947374	4936.202262	7.354163	-0.042182	3.815355
210.058693	4944.202675	7.359168	-0.042208	3.818314
210.336090	4952.231244	7.364173	-0.042265	3.821284
210.406249	4960.221167	7.369178	-0.042284	3.824234
210.411693	4968.257357	7.374182	-0.042290	3.827197
210.764549	4976.294738	7.379187	-0.042361	3.830166
210.822413	4984.313409	7.384192	-0.042377	3.833119
211.019484	4992.361120	7.389197	-0.042419	3.836083
211.306066	5000.381297	7.394202	-0.042477	3.839037
211.427458	5008.366734	7.399206	-0.042505	3.841972
211.818232	5016.341812	7.404211	-0.042583	3.844907
212.038049	5024.369155	7.409216	-0.042629	3.847855
211.978826	5032.471702	7.414221	-0.042623	3.850823
212.164092	5040.490401	7.419226	-0.042663	3.853762
212.296481	5048.548910	7.424230	-0.042693	3.856713
212.868509	5056.508735	7.429235	-0.042805	3.859635
212.883559	5064.539892	7.434240	-0.042813	3.862569
213.122725	5072.577980	7.439245	-0.042862	3.865507
213.312666	5080.604376	7.444250	-0.042903	3.868439
213.716558	5088.626412	7.449254	-0.042983	3.871370
214.007476	5096.897405	7.454259	-0.043043	3.874388
214.223045	5104.798751	7.459264	-0.043088	3.877267
214.821048	5112.740040	7.464269	-0.043205	3.880166
215.282925	5120.688658	7.469274	-0.043296	3.883063
215.215264	5128.702065	7.474278	-0.043289	3.885971
215.677865	5136.728274	7.479283	-0.043380	3.888892
215.817296	5144.750782	7.484288	-0.043411	3.891803
215.859417	5152.828364	7.489293	-0.043424	3.894730
215.990295	5160.824648	7.494298	-0.043454	3.897627
216.473655	5168.788143	7.499302	-0.043549	3.900516
216.407388	5176.897310	7.504307	-0.043542	3.903446
216.780319	5184.846645	7.509312	-0.043617	3.906324
216.911107	5192.883517	7.514317	-0.043646	3.909227
217.132697	5200.913181	7.519322	-0.043693	3.912126
217.173377	5208.968406	7.524326	-0.043705	3.915030
217.529650	5216.953975	7.529331	-0.043777	3.917912
217.585189	5224.977955	7.534336	-0.043793	3.920800
217.666140	5232.979691	7.539341	-0.043813	3.923678
217.826558	5241.001664	7.544346	-0.043848	3.926563
218.357218	5248.939148	7.549350	-0.043952	3.929423
218.490031	5257.018847	7.554355	-0.043982	3.932324
218.664069	5265.026765	7.559360	-0.044019	3.935197
219.040994	5273.069965	7.564365	-0.044095	3.938085
218.816959	5281.119615	7.569370	-0.044058	3.940963
218.799830	5289.082111	7.574374	-0.044060	3.943811
218.992068	5297.166976	7.579379	-0.044101	3.946704
219.196429	5305.156727	7.584384	-0.044145	3.949561
219.544561	5313.192744	7.589389	-0.044215	3.952435
219.616958	5321.235620	7.594394	-0.044233	3.955305
219.751712	5329.262144	7.599398	-0.044264	3.958168
220.024742	5337.258205	7.604403	-0.044320	3.961020
220.194903	5345.176349	7.609408	-0.044357	3.963841
220.793053	5353.180310	7.614413	-0.044473	3.966697
220.881805	5361.221059	7.619418	-0.044495	3.969556
221.110943	5369.257622	7.624422	-0.044543	3.972413
221.392736	5377.324929	7.629427	-0.044601	3.975281
221.587219	5385.300032	7.634432	-0.044642	3.978112
221.816521	5393.326909	7.639437	-0.044690	3.980960
221.876145	5401.366492	7.644442	-0.044706	3.983807
221.902937	5409.400110	7.649446	-0.044716	3.986650
222.204158	5417.448277	7.654451	-0.044778	3.989500
222.183132	5425.476176	7.659456	-0.044779	3.992337
222.310920	5433.524344	7.664461	-0.044808	3.995180
222.698290	5441.547253	7.669466	-0.044885	3.998017
222.492429	5449.524424	7.674470	-0.044852	4.000826
222.970749	5457.513214	7.679475	-0.044947	4.003648
222.921840	5465.565657	7.684480	-0.044943	4.006482
223.074161	5473.625622	7.689485	-0.044976	4.009320
223.137160	5481.658844	7.694490	-0.044993	4.012145
223.465956	5489.650658	7.699494	-0.045060	4.014958
223.918877	5497.695345	7.704499	-0.045149	4.017789
223.807852	5505.673137	7.709504	-0.045134	4.020586
224.197263	5513.667077	7.714509	-0.045211	4.023394
224.272001	5521.699807	7.719514	-0.045231	4.026209
224.674062	5529.657392	7.724518	-0.045311	4.029001
224.798541	5537.797563	7.729523	-0.045339	4.031850
225.085560	5545.846485	7.734528	-0.045398	4.034668
225.314620	5553.852629	7.739533	-0.045446	4.037468
225.486423	5561.825667	7.744538	-0.045483	4.040254
225.398673	5569.815049	7.749542	-0.045472	4.043040
225.797114	5577.788950	7.754547	-0.045551	4.045825
226.118337	5585.795899	7.759552	-0.045616	4.048619
226.335098	5593.865723	7.764557	-0.045662	4.051431
226.266618	5601.925924	7.769562	-0.045654	4.054234
226.491046	5609.945685	7.774566	-0.045701	4.057025
226.732603	5617.914641	7.779571	-0.045751	4.059797
226.707780	5625.949310	7.784576	-0.045752	4.062586
227.353918	5633.910515	7.789581	-0.045877	4.065357
227.673666	5641.949845	7.794586	-0.045942	4.068148
227.885874	5649.972943	7.799590	-0.045987	4.070930
228.213949	5658.058417	7.804595	-0.046053	4.073734
228.463091	5666.060613	7.809600	-0.046105	4.076506
228.433567	5674.053914	7.814605	-0.046105	4.079269
228.797104	5682.060013	7.819610	-0.046178	4.082039
229.235138	5690.001900	7.824614	-0.046264	4.084787
229.574845	5698.109699	7.829619	-0.046333	4.087589
229.499223	5706.099542	7.834624	-0.046324	4.090342
229.731108	5714.174635	7.839629	-0.046372	4.093128
229.862040	5722.230115	7.844634	-0.046402	4.095903
230.230054	5730.169666	7.849638	-0.046476	4.098639
230.710805	5738.204941	7.854643	-0.046570	4.101408
230.694108	5746.186159	7.859648	-0.046572	4.104150
230.929498	5754.232528	7.864653	-0.046622	4.106916
231.354198	5762.226502	7.869658	-0.046706	4.109664
231.428707	5770.309852	7.874662	-0.046725	4.112437
231.649018	5778.360586	7.879667	-0.046771	4.115198
231.560951	5786.373254	7.884672	-0.046760	4.117941
231.849432	5794.296470	7.889677	-0.046819	4.120656
232.082351	5802.360359	7.894682	-0.046867	4.123416
232.129634	5810.333092	7.899686	-0.046881	4.126141
232.402585	5818.381785	7.904691	-0.046938	4.128894
232.487544	5826.450818	7.909696	-0.046959	4.131648
232.713301	5834.480064	7.914701	-0.047006	4.134390
232.790378	5842.548317	7.919706	-0.047025	4.137140
233.234179	5850.451586	7.924710	-0.047113	4.139837
233.425866	5858.536778	7.929715	-0.047154	4.142592
233.365735	5866.487307	7.934720	-0.047148	4.145295
233.570698	5874.589266	7.939725	-0.047192	4.148052
234.103757	5882.537601	7.944730	-0.047296	4.150758
234.057023	5890.589950	7.949734	-0.047293	4.153491
234.322723	5898.651884	7.954739	-0.047347	4.156229
234.414026	5906.637530	7.959744	-0.047369	4.158937
234.574696	5914.632589	7.964749	-0.047405	4.161648
234.470953	5922.655447	7.969754	-0.047390	4.164363
234.673154	5930.670757	7.974758	-0.047433	4.167077
235.028805	5938.699339	7.979763	-0.047505	4.169796
235.157428	5946.703663	7.984768	-0.047534	4.172502
235.709109	5954.735762	7.989773	-0.047642	4.175220
235.650705	5962.739077	7.994778	-0.047636	4.177921
235.931991	5970.719212	7.999782	-0.047694	4.180615
235.920838	5978.837982	8.004787	-0.047697	4.183351
235.656117	5986.850379	8.009792	-0.047653	4.186047
235.985077	5994.862396	8.014797	-0.047719	4.188747
236.399755	6002.823231	8.019802	-0.047802	4.191429
236.488821	6010.916386	8.024806	-0.047824	4.194151
236.873531	6018.943550	8.029811	-0.047900	4.196851
236.758240	6026.852574	8.034816	-0.047884	4.199505
236.936059	6034.910406	8.039821	-0.047923	4.202210
237.433069	6042.843821	8.044826	-0.048020	4.204875
237.286325	6050.929272	8.049830	-0.047998	4.207583
237.493578	6058.983331	8.054835	-0.048042	4.210282
237.290292	6067.055604	8.059840	-0.048009	4.212981
237.522376	6074.998916	8.064845	-0.048058	4.215640
237.849076	6082.990399	8.069850	-0.048124	4.218314
238.257493	6090.973528	8.074854	-0.048205	4.220984
238.331220	6099.078089	8.079859	-0.048224	4.223690
238.562439	6107.058908	8.084864	-0.048272	4.226354
239.324643	6115.025258	8.089869	-0.048419	4.229017
239.553353	6123.056835	8.094874	-0.048467	4.231695
239.583101	6131.129130	8.099878	-0.048478	4.234383
239.756900	6139.205428	8.104883	-0.048516	4.237071
240.293416	6147.116416	8.109888	-0.048621	4.239707
240.759699	6155.123742	8.114893	-0.048713	4.242371
240.905701	6163.132698	8.119898	-0.048745	4.245032
241.275311	6171.177471	8.124902	-0.048819	4.247705
241.463945	6179.191781	8.129907	-0.048859	4.250365
241.573094	6187.250977	8.134912	-0.048885	4.253037
241.764355	6195.278264	8.139917	-0.048926	4.255698
241.816796	6203.318978	8.144922	-0.048941	4.258360
241.900974	6211.304462	8.149926	-0.048962	4.261002
241.667087	6219.414532	8.154931	-0.048923	4.263682
241.788121	6227.386402	8.159936	-0.048951	4.266317
241.688506	6235.427446	8.164941	-0.048938	4.268971
242.099933	6243.381212	8.169946	-0.049020	4.271599
242.596761	6251.373922	8.174950	-0.049117	4.274239
242.673608	6259.477803	8.179955	-0.049137	4.276911
242.714561	6267.387604	8.184960	-0.049150	4.279516
243.042562	6275.471776	8.189965	-0.049216	4.282180
243.441174	6283.381906	8.194970	-0.049295	4.284785
243.438756	6291.489888	8.199974	-0.049300	4.287451
243.881769	6299.468854	8.204979	-0.049388	4.290076
243.763770	6307.560171	8.209984	-0.049371	4.292732
243.886119	6315.568088	8.214989	-0.049399	4.295360
243.840778	6323.626724	8.219994	-0.049396	4.298003
244.022966	6331.588883	8.224998	-0.049435	4.300614
244.478507	6339.588876	8.230003	-0.049525	4.303237
244.682200	6347.567149	8.235008	-0.049568	4.305851
244.873354	6355.617460	8.240013	-0.049609	4.308486
244.767653	6363.690780	8.245018	-0.049595	4.311124
244.851683	6371.696056	8.250022	-0.049616	4.313740
245.383704	6379.701332	8.255027	-0.049720	4.316358
245.514026	6387.654264	8.260032	-0.049749	4.318955
245.704300	6395.694076	8.265037	-0.049790	4.321578
245.980721	6403.716926	8.270042	-0.049847	4.324195
245.964902	6411.739338	8.275046	-0.049849	4.326808
246.482751	6419.706666	8.280051	-0.049950	4.329405
246.417945	6427.780171	8.285056	-0.049944	4.332031
246.713875	6435.790747	8.290061	-0.050004	4.334638
246.874136	6443.842628	8.295066	-0.050039	4.337255
246.970183	6451.827635	8.300070	-0.050062	4.339849
247.186133	6459.859371	8.305075	-0.050108	4.342457
247.629934	6467.807835	8.310080	-0.050195	4.345038
247.755468	6475.863678	8.315085	-0.050224	4.347650
247.802742	6483.891213	8.320090	-0.050238	4.350251
247.938678	6491.969170	8.325094	-0.050269	4.352868
248.031380	6500.056718	8.330099	-0.050291	4.355485
248.216790	6508.019023	8.335104	-0.050331	4.358061
248.199720	6515.986922	8.340109	-0.050333	4.360636
248.462877	6523.944797	8.345114	-0.050387	4.363208
248.734032	6531.922817	8.350118	-0.050443	4.365785
249.134821	6540.011793	8.355123	-0.050523	4.368397
249.073161	6548.047033	8.360128	-0.050516	4.370987
249.335766	6556.020357	8.365133	-0.050570	4.373558
249.628595	6564.100764	8.370138	-0.050630	4.376161
249.408851	6572.099676	8.375142	-0.050594	4.378735
249.757713	6580.099542	8.380147	-0.050665	4.381310
249.830630	6588.083557	8.385152	-0.050683	4.383877
250.164003	6596.122477	8.390157	-0.050751	4.386461
250.635759	6604.085266	8.395162	-0.050844	4.389020
250.620080	6612.120023	8.400166	-0.050846	4.391598
250.681378	6620.227433	8.405171	-0.050863	4.394199
250.730851	6628.240475	8.410176	-0.050877	4.396767
250.929875	6636.190617	8.415181	-0.050919	4.399315
251.228279	6644.250282	8.420186	-0.050980	4.401896
251.303074	6652.184421	8.425190	-0.050999	4.404435
251.662533	6660.285012	8.430195	-0.051071	4.407027
251.784619	6668.270843	8.435200	-0.051099	4.409579
252.083751	6676.301842	8.440205	-0.051160	4.412146
252.343205	6684.337228	8.445210	-0.051214	4.414712
252.425607	6692.358333	8.450214	-0.051234	4.417271
252.533888	6700.321084	8.455219	-0.051260	4.419810
252.730404	6708.403901	8.460224	-0.051302	4.422386
252.990878	6716.372002	8.465229	-0.051355	4.424925
253.093870	6724.491106	8.470234	-0.051380	4.427509
253.284201	6732.454815	8.475238	-0.051420	4.430043
253.618175	6740.516626	8.480243	-0.051488	4.432607
253.772229	6748.507853	8.485248	-0.051522	4.435146
253.704081	6756.495661	8.490253	-0.051514	4.437682
254.263910	6764.490210	8.495258	-0.051624	4.440222
254.511282	6772.489373	8.500262	-0.051675	4.442759
254.411780	6780.550507	8.505267	-0.051662	4.445314
254.644341	6788.567050	8.510272	-0.051710	4.447855
254.826737	6796.567149	8.515277	-0.051749	4.450388
254.937978	6804.620056	8.520282	-0.051775	4.452937
255.005398	6812.617873	8.525286	-0.051793	4.455466
255.240879	6820.623394	8.530291	-0.051842	4.457997
255.416966	6828.599594	8.535296	-0.051880	4.460517
255.578147	6836.598342	8.540301	-0.051915	4.463043
255.829793	6844.656197	8.545306	-0.051967	4.465586
256.063709	6852.697144	8.550310	-0.052016	4.468122
256.124938	6860.689957	8.555315	-0.052033	4.470641
256.216714	6868.772282	8.560320	-0.052055	4.473187
256.516436	6876.747180	8.565325	-0.052116	4.475699
256.764873	6884.778772	8.570330	-0.052168	4.478226
256.827968	6892.732264	8.575335	-0.052184	4.480727
257.184754	6900.766140	8.580339	-0.052256	4.483253
257.088605	6908.759891	8.585344	-0.052243	4.485763
257.500423	6916.766731	8.590349	-0.052325	4.488278
257.805018	6924.838844	8.595354	-0.052387	4.490811
257.738688	6932.853890	8.600359	-0.052380	4.493324
257.926647	6940.911270	8.605363	-0.052420	4.495849
258.007333	6948.921236	8.610368	-0.052441	4.498358
258.443437	6956.838282	8.615373	-0.052527	4.500837
258.733093	6964.904684	8.620378	-0.052586	4.503362
258.761206	6972.897679	8.625383	-0.052597	4.505861
259.006973	6980.958593	8.630387	-0.052648	4.508380
259.051486	6988.966469	8.635392	-0.052661	4.510881
259.356782	6997.003138	8.640397	-0.052723	4.513390
259.603381	7005.065800	8.645402	-0.052774	4.515906
259.909040	7013.013511	8.650407	-0.052836	4.518385
260.014411	7021.022014	8.655411	-0.052861	4.520880
260.112596	7029.009964	8.660416	-0.052885	4.523368
260.427806	7037.028253	8.665421	-0.052949	4.525865
260.490098	7045.046420	8.670426	-0.052965	4.528359
260.689071	7053.041224	8.675431	-0.053008	4.530845
260.942105	7061.106568	8.680435	-0.053060	4.533352
261.007718	7069.119046	8.685440	-0.053077	4.535840
261.132529	7077.119593	8.690445	-0.053106	4.538324
261.499563	7085.144674	8.695450	-0.053179	4.540814
261.626583	7093.150122	8.700455	-0.053208	4.543296
261.888039	7101.174595	8.705459	-0.053262	4.545783
262.013900	7109.197020	8.710464	-0.053291	4.548268
262.288220	7117.168887	8.715469	-0.053347	4.550736
262.544586	7125.270426	8.720474	-0.053400	4.553243
262.503879	7133.255262	8.725479	-0.053398	4.555712
262.690190	7141.282155	8.730483	-0.053438	4.558192
262.903131	7149.267929	8.735488	-0.053483	4.560659
263.036814	7157.278553	8.740493	-0.053513	4.563132
263.177381	7165.283445	8.745498	-0.053544	4.565602
263.365468	7173.274403	8.750503	-0.053584	4.568066
263.717651	7181.365699	8.755507	-0.053655	4.570560
263.868669	7189.401085	8.760512	-0.053688	4.573035
264.056199	7197.416488	8.765517	-0.053729	4.575503
264.404195	7205.461456	8.770522	-0.053799	4.577978
264.335513	7213.392594	8.775527	-0.053791	4.580417
264.528531	7221.456724	8.780531	-0.053832	4.582896
264.564558	7229.449180	8.785536	-0.053844	4.585351
264.665993	7237.459127	8.790541	-0.053868	4.587810
264.869976	7245.496787	8.795546	-0.053911	4.590276
264.979834	7253.548040	8.800551	-0.053937	4.592745
265.288032	7261.563945	8.805555	-0.054000	4.595202
265.391343	7269.584227	8.810560	-0.054024	4.597659
265.564926	7277.520144	8.815565	-0.054062	4.600089
265.927856	7285.579839	8.820570	-0.054134	4.602556
266.036399	7293.504947	8.825575	-0.054160	4.604980
266.169663	7301.590603	8.830579	-0.054190	4.607451
266.637813	7309.610535	8.835584	-0.054282	4.609901
266.574423	7317.623961	8.840589	-0.054276	4.612348
266.645278	7325.658210	8.845594	-0.054294	4.614801
266.951878	7333.643951	8.850599	-0.054356	4.617236
267.280885	7341.657641	8.855603	-0.054423	4.619679
267.446931	7349.688678	8.860608	-0.054459	4.622126
267.419850	7357.620021	8.865613	-0.054459	4.624542
267.847100	7365.753654	8.870618	-0.054544	4.627017
267.963054	7373.724666	8.875623	-0.054571	4.629442
267.838752	7381.760822	8.880627	-0.054553	4.631886
268.157986	7389.774835	8.885632	-0.054617	4.634321
268.274320	7397.824389	8.890637	-0.054644	4.636766
268.526996	7405.797462	8.895642	-0.054697	4.639186
268.551653	7413.827471	8.900647	-0.054706	4.641622
268.781213	7421.795589	8.905651	-0.054754	4.644038
268.964171	7429.822368	8.910656	-0.054794	4.646471
269.085637	7437.842857	8.915661	-0.054821	4.648901
269.301655	7445.892779	8.920666	-0.054867	4.651338
269.363343	7453.874050	8.925671	-0.054884	4.653753
269.668163	7461.926775	8.930675	-0.054946	4.656188
269.932441	7469.900993	8.935680	-0.055000	4.658598
269.937544	7477.933885	8.940685	-0.055006	4.661025
270.014139	7485.959994	8.945690	-0.055026	4.663449
270.128644	7493.880859	8.950695	-0.055052	4.665839
270.632133	7501.984117	8.955699	-0.055151	4.668283
270.599329	7510.008801	8.960704	-0.055150	4.670702
270.585480	7518.059522	8.965709	-0.055153	4.673129
270.877156	7526.117452	8.970714	-0.055212	4.675555
270.933326	7534.066078	8.975719	-0.055228	4.677948
271.094560	7542.049625	8.980723	-0.055263	4.680349
271.283190	7550.080114	8.985728	-0.055304	4.682764
271.311549	7557.995219	8.990733	-0.055314	4.685143
271.568029	7566.123972	8.995738	-0.055367	4.687584
271.676712	7574.046887	9.000743	-0.055392	4.689963
272.041454	7582.165275	9.005747	-0.055466	4.692399
272.179489	7590.130032	9.010752	-0.055497	4.694787
272.244994	7598.173308	9.015757	-0.055514	4.697198
272.567079	7606.136417	9.020762	-0.055579	4.699583
272.688705	7614.201030	9.025767	-0.055607	4.701998
272.946284	7622.128118	9.030771	-0.055660	4.704370
273.021831	7630.214240	9.035776	-0.055679	4.706789
273.190099	7638.231266	9.040781	-0.055716	4.709186
273.596361	7646.253653	9.045786	-0.055797	4.711583
273.570935	7654.295991	9.050791	-0.055797	4.713985
273.994552	7662.337434	9.055795	-0.055882	4.716385
274.069562	7670.262437	9.060800	-0.055901	4.718749
274.283863	7678.264076	9.065805	-0.055946	4.721135
274.539485	7686.331043	9.070810	-0.055999	4.723539
274.685035	7694.311968	9.075815	-0.056031	4.725916
274.838070	7702.399825	9.080819	-0.056065	4.728324
274.985491	7710.415219	9.085824	-0.056097	4.730710
275.231697	7718.365500	9.090829	-0.056148	4.733074
275.372433	7726.471993	9.095834	-0.056180	4.735484
275.352948	7734.433707	9.100839	-0.056181	4.737850
275.623236	7742.464850	9.105843	-0.056237	4.740234
276.063191	7750.471682	9.110848	-0.056324	4.742610
275.895165	7758.410042	9.115853	-0.056298	4.744966
276.317595	7766.505964	9.120858	-0.056382	4.747366
276.341490	7774.484202	9.125863	-0.056391	4.749731
276.451182	7782.560282	9.130867	-0.056417	4.752123
276.719120	7790.641483	9.135872	-0.056472	4.754515
276.646863	7798.583113	9.140877	-0.056464	4.756866
276.965156	7806.551820	9.145882	-0.056528	4.759222
276.955471	7814.572961	9.150887	-0.056532	4.761594
277.203632	7822.571014	9.155891	-0.056583	4.763957
277.202078	7830.611939	9.160896	-0.056588	4.766332
277.347839	7838.570123	9.165901	-0.056621	4.768681
277.680902	7846.659855	9.170906	-0.056688	4.771067
277.842304	7854.632693	9.175911	-0.056723	4.773418
278.008901	7862.693292	9.180915	-0.056759	4.775793
278.284800	7870.663166	9.185920	-0.056816	4.778140
278.401985	7878.656937	9.190925	-0.056843	4.780494
278.684052	7886.720883	9.195930	-0.056901	4.782866
278.709398	7894.680942	9.200935	-0.056911	4.785208
279.114158	7902.773011	9.205939	-0.056991	4.787586
279.080329	7910.791094	9.210944	-0.056990	4.789943
279.031430	7918.788428	9.215949	-0.056986	4.792292
279.203181	7926.813486	9.220954	-0.057023	4.794648
279.383635	7934.852284	9.225959	-0.057062	4.797006
279.680785	7942.730994	9.230963	-0.057123	4.799316
279.798590	7950.861949	9.235968	-0.057150	4.801699
279.972102	7958.795481	9.240973	-0.057187	4.804023
280.120869	7966.867901	9.245978	-0.057220	4.806387
280.091505	7974.837775	9.250983	-0.057220	4.808720
280.649762	7982.907294	9.255987	-0.057329	4.811079
280.605724	7990.406460	9.260992	-0.057326	4.813272
280.724883	7994.999288	9.265997	-0.057351	4.814614

280.910565	7997.374843	9.271002	-0.057387	4.815308
281.298843	7998.716054	9.276007	-0.057460	4.815698
281.086411	7999.266642	9.281011	-0.057421	4.815860
280.999643	7999.804563	9.286016	-0.057405	4.816017
281.200637	7999.803931	9.291021	-0.057443	4.816016
281.343927	7999.785160	9.296026	-0.057469	4.816010
281.223858	7999.747729	9.301031	-0.057447	4.816000
281.289867	7999.742514	9.306035	-0.057459	4.815998
281.365428	7999.770590	9.311040	-0.057473	4.816005
281.427605	7999.700138	9.316045	-0.057485	4.815985
281.616515	7999.791163	9.321050	-0.057520	4.816010
281.597700	7999.933979	9.326055	-0.057517	4.816052
281.773410	7999.889087	9.331059	-0.057549	4.816038
281.699156	7999.861032	9.336064	-0.057536	4.816030
281.737554	7999.974972	9.341069	-0.057543	4.816063
281.981368	7999.896059	9.346074	-0.057588	4.816039
281.745106	7999.971902	9.351079	-0.057544	4.816062
282.006198	7999.866593	9.356083	-0.057593	4.816030
282.203944	7999.925731	9.361088	-0.057630	4.816046
281.965552	7999.951323	9.366093	-0.057585	4.816055
282.020035	7999.938421	9.371098	-0.057595	4.816051
281.908768	7999.916104	9.376103	-0.057575	4.816045
282.163106	7999.817084	9.381107	-0.057622	4.816015
282.016878	7999.947976	9.386112	-0.057595	4.816054
282.007651	7999.896527	9.391117	-0.057593	4.816039
282.216065	7999.826588	9.396122	-0.057632	4.816017
282.238952	7999.888966	9.401127	-0.057636	4.816035
282.309250	7999.893445	9.406131	-0.057649	4.816036
282.264598	7999.895840	9.411136	-0.057641	4.816037
282.331786	7999.853254	9.416141	-0.057653	4.816025
282.247798	7999.889123	9.421146	-0.057638	4.816035
282.225083	7999.911146	9.426151	-0.057633	4.816042
282.647947	7999.873940	9.431155	-0.057712	4.816029
282.245887	7999.931820	9.436160	-0.057637	4.816048
282.513951	7999.855484	9.441165	-0.057687	4.816024
282.648824	7999.913483	9.446170	-0.057712	4.816040
282.375112	7999.888221	9.451175	-0.057661	4.816035
282.416059	7999.887894	9.456179	-0.057669	4.816034
282.536850	7999.897561	9.461184	-0.057691	4.816036
282.615419	7999.807105	9.466189	-0.057706	4.816010
282.648492	7999.923088	9.471194	-0.057712	4.816043
282.487403	7999.913756	9.476199	-0.057682	4.816041
282.561047	7999.897996	9.481203	-0.057696	4.816036
282.659754	7999.824999	9.486208	-0.057714	4.816015
282.531021	7999.949800	9.491213	-0.057690	4.816052
282.723680	7999.778080	9.496218	-0.057726	4.816000
282.652963	7999.974445	9.501223	-0.057713	4.816058
282.669124	7999.870037	9.506227	-0.057716	4.816028
282.967352	7999.888264	9.511232	-0.057771	4.816031
282.876608	7999.893028	9.516237	-0.057754	4.816033
283.053755	7999.819316	9.521242	-0.057787	4.816011
282.909885	7999.890424	9.526247	-0.057761	4.816032
282.772691	7999.865500	9.531251	-0.057735	4.816026
282.814398	7999.984845	9.536256	-0.057743	4.816060
282.934062	7999.859877	9.541261	-0.057765	4.816023
283.104776	7999.909981	9.546266	-0.057797	4.816037
282.981189	7999.882097	9.551271	-0.057774	4.816030
282.983032	7999.849010	9.556275	-0.057774	4.816020
283.064083	7999.910308	9.561280	-0.057789	4.816037
283.069466	7999.891174	9.566285	-0.057790	4.816032
282.806947	7999.871456	9.571290	-0.057741	4.816027
282.853291	7999.960970	9.576295	-0.057750	4.816053
283.118275	7999.858937	9.581299	-0.057799	4.816022
282.989587	7999.903611	9.586304	-0.057775	4.816036
282.852592	7999.881895	9.591309	-0.057750	4.816030
282.971107	7999.830624	9.596314	-0.057772	4.816015
282.977665	7999.902324	9.601319	-0.057773	4.816035
282.994391	7999.816088	9.606323	-0.057776	4.816010
283.157729	7999.892767	9.611328	-0.057807	4.816032
283.185425	7999.898610	9.616333	-0.057812	4.816033
283.058773	7999.825799	9.621338	-0.057788	4.816013
283.147342	7999.924627	9.626343	-0.057805	4.816041
283.059779	7999.821542	9.631347	-0.057788	4.816011
283.321399	7999.917098	9.636352	-0.057837	4.816038
283.139495	7999.829396	9.641357	-0.057803	4.816013
283.249594	7999.839939	9.646362	-0.057824	4.816016
283.184085	7999.970161	9.651367	-0.057812	4.816054
283.150124	7999.792193	9.656371	-0.057805	4.816002
283.121093	7999.934828	9.661376	-0.057800	4.816044
283.238354	7999.867509	9.666381	-0.057822	4.816024
283.240160	7999.882498	9.671386	-0.057822	4.816028
283.200968	7999.904223	9.676391	-0.057815	4.816035
283.258763	7999.903133	9.681395	-0.057825	4.816034
283.331344	7999.906585	9.686400	-0.057839	4.816035
283.084360	7999.961935	9.691405	-0.057793	4.816052
283.269100	7999.837078	9.696410	-0.057827	4.816015
283.517342	7999.915298	9.701415	-0.057873	4.816036
283.459778	7999.789252	9.706419	-0.057863	4.816000
283.328609	7999.973840	9.711424	-0.057838	4.816054
283.307062	7999.804643	9.716429	-0.057834	4.816005
283.170126	7999.922886	9.721434	-0.057809	4.816040
283.203072	7999.880747	9.726439	-0.057815	4.816028
283.341594	7999.869370	9.731443	-0.057841	4.816024
283.394356	7999.951523	9.736448	-0.057851	4.816048
283.279810	7999.773162	9.741453	-0.057829	4.815996
283.434870	7999.909520	9.746458	-0.057858	4.816035
283.515951	7999.909922	9.751463	-0.057873	4.816035
283.685055	7999.910851	9.756467	-0.057905	4.816034
283.726927	7999.900926	9.761472	-0.057912	4.816031
283.666189	7999.790847	9.766477	-0.057901	4.815999
283.694420	7999.928113	9.771482	-0.057906	4.816039
283.687259	7999.862810	9.776487	-0.057905	4.816020
283.460326	7999.862967	9.781491	-0.057863	4.816021
283.482296	7999.932809	9.786496	-0.057867	4.816042
283.376253	7999.869987	9.791501	-0.057847	4.816024
283.596831	7999.910312	9.796506	-0.057888	4.816035
283.484179	7999.886900	9.801511	-0.057867	4.816028
283.497414	7999.914917	9.806515	-0.057870	4.816036
283.457379	7999.847950	9.811520	-0.057862	4.816017
283.409142	7999.879126	9.816525	-0.057853	4.816026
283.547293	7999.808981	9.821530	-0.057879	4.816005
283.274917	7999.933314	9.826535	-0.057828	4.816043
283.583631	7999.807501	9.831539	-0.057885	4.816005
283.554109	7999.940513	9.836544	-0.057880	4.816044
283.451637	7999.800832	9.841549	-0.057861	4.816003
283.671040	7999.914854	9.846554	-0.057902	4.816035
283.847389	7999.836854	9.851559	-0.057935	4.816012
283.591540	7999.887769	9.856563	-0.057887	4.816028
283.559705	7999.963046	9.861568	-0.057881	4.816050
283.702145	7999.872679	9.866573	-0.057908	4.816023
283.784558	7999.851737	9.871578	-0.057923	4.816016
283.717511	7999.987274	9.876583	-0.057910	4.816056
283.542503	7999.792857	9.881587	-0.057878	4.816000
283.661872	7999.819594	9.886592	-0.057900	4.816008
283.788591	7999.894542	9.891597	-0.057924	4.816029
283.615620	7999.829437	9.896602	-0.057891	4.816011
283.799818	7999.934274	9.901607	-0.057926	4.816040
283.659899	7999.804597	9.906611	-0.057900	4.816003
283.643315	7999.968828	9.911616	-0.057897	4.816051
283.758667	7999.810660	9.916621	-0.057918	4.816005
283.948861	7999.931633	9.921626	-0.057953	4.816039
283.784654	7999.832497	9.926631	-0.057923	4.816011
283.682893	7999.893686	9.931635	-0.057904	4.816029
283.931149	7999.885367	9.936640	-0.057950	4.816025
283.735394	7999.877542	9.941645	-0.057914	4.816024
283.585764	7999.790424	9.946650	-0.057886	4.816000
283.878293	7999.932484	9.951655	-0.057940	4.816040
283.839838	7999.900802	9.956659	-0.057933	4.816030
283.868936	7999.865003	9.961664	-0.057938	4.816020
283.680217	7999.823117	9.966669	-0.057903	4.816009
283.990619	7999.866140	9.971674	-0.057961	4.816020
283.757089	7999.820236	9.976679	-0.057918	4.816007
283.650261	7999.921931	9.981683	-0.057898	4.816038
283.742111	7999.854151	9.986688	-0.057915	4.816017
283.813050	7999.922746	9.991693	-0.057928	4.816037
283.772552	7999.905984	9.996698	-0.057920	4.816032
283.551337	7999.866714	10.001703	-0.057879	4.816022
283.589039	7999.850303	10.006707	-0.057886	4.816017
283.963766	7999.846415	10.011712	-0.057956	4.816014
283.781993	7999.983077	10.016717	-0.057922	4.816055
283.885029	7999.803317	10.021722	-0.057941	4.816002
283.734411	7999.901013	10.026727	-0.057913	4.816031
283.597393	7999.855791	10.031731	-0.057888	4.816019
283.988178	7999.852195	10.036736	-0.057960	4.816015
283.912939	7999.970490	10.041741	-0.057947	4.816050
283.774124	7999.779933	10.046746	-0.057921	4.815995
283.727912	7999.921190	10.051751	-0.057912	4.816037
283.630469	7999.916217	10.056755	-0.057894	4.816036
283.781124	7999.874076	10.061760	-0.057922	4.816023
283.732845	7999.954397	10.066765	-0.057913	4.816047
283.875802	7999.828782	10.071770	-0.057939	4.816009
283.602868	7999.880456	10.076775	-0.057889	4.816026
283.546307	7999.916822	10.081779	-0.057878	4.816037
283.814207	7999.820183	10.086784	-0.057928	4.816007
284.046914	7999.883165	10.091789	-0.057971	4.816024
283.979492	7999.788991	10.096794	-0.057959	4.815997
283.799276	7999.914997	10.101799	-0.057925	4.816035
283.932960	7999.968704	10.106803	-0.057950	4.816050
284.011977	7999.809877	10.111808	-0.057965	4.816003
283.728846	7999.953247	10.116813	-0.057912	4.816046
283.943626	7999.786199	10.121818	-0.057952	4.815996
283.886703	8000.038376	10.126823	-0.057942	4.816070
283.866743	7999.992072	10.131827	-0.057938	4.816057
284.037764	7999.991969	10.136832	-0.057970	4.816056
283.973767	7999.952344	10.141837	-0.057958	4.816045
284.049023	7999.775285	10.146842	-0.057972	4.815993
284.035927	7999.945991	10.151847	-0.057969	4.816043
284.043930	7999.859595	10.156851	-0.057971	4.816017
284.215602	7999.800741	10.161856	-0.058003	4.815999
284.090129	7999.899962	10.166861	-0.057979	4.816029
284.279057	7999.813642	10.171866	-0.058014	4.816003
284.315536	7999.944649	10.176871	-0.058021	4.816041
284.396934	7999.794411	10.181875	-0.058036	4.815996
284.326239	7999.917063	10.186880	-0.058023	4.816033
284.191035	7999.869736	10.191885	-0.057998	4.816020
284.239774	7999.828951	10.196890	-0.058007	4.816007
284.200646	7999.959654	10.201895	-0.058000	4.816046
284.212873	7999.856240	10.206899	-0.058002	4.816015
284.253873	7999.968097	10.211904	-0.058010	4.816048
284.268387	7999.862587	10.216909	-0.058012	4.816017
284.144557	7999.821877	10.221914	-0.057989	4.816006
284.433852	7999.907255	10.226919	-0.058043	4.816029
284.437548	7999.861380	10.231923	-0.058044	4.816016
284.424335	7999.788487	10.236928	-0.058041	4.815995
284.334729	8000.021911	10.241933	-0.058025	4.816063
284.393291	7999.824248	10.246938	-0.058035	4.816005
284.346345	7999.800959	10.251943	-0.058027	4.815999
284.497621	7999.873149	10.256947	-0.058055	4.816019
284.691156	7999.787981	10.261952	-0.058091	4.815993
284.472131	7999.938927	10.266957	-0.058050	4.816038
284.348548	7999.782833	10.271962	-0.058027	4.815993
284.648146	7999.970966	10.276967	-0.058083	4.816047
284.358267	7999.894121	10.281971	-0.058029	4.816026
284.451307	7999.838114	10.286976	-0.058046	4.816009
284.426666	7999.864377	10.291981	-0.058042	4.816017
284.653553	7999.778746	10.296986	-0.058084	4.815990
284.457577	7999.901262	10.301991	-0.058047	4.816027
284.411035	7999.867295	10.306995	-0.058039	4.816018
284.524165	7999.887510	10.312000	-0.058060	4.816023
284.331827	7999.884020	10.317005	-0.058024	4.816023
284.370016	7999.878301	10.322010	-0.058031	4.816021
284.322890	7999.883856	10.327015	-0.058022	4.816023
284.294472	7999.911118	10.332019	-0.058017	4.816031
284.410457	7999.871553	10.337024	-0.058039	4.816019
284.526495	8000.004004	10.342029	-0.058060	4.816057
284.651107	7999.872712	10.347034	-0.058083	4.816018
284.401158	7999.899160	10.352039	-0.058037	4.816027
284.476928	7999.897329	10.357043	-0.058051	4.816026
284.537130	7999.859957	10.362048	-0.058062	4.816015
284.463171	7999.971867	10.367053	-0.058048	4.816048
284.511378	7999.888336	10.372058	-0.058057	4.816023
284.389509	7999.886124	10.377063	-0.058035	4.816023
284.311298	7999.872951	10.382067	-0.058020	4.816020
284.500672	7999.883865	10.387072	-0.058055	4.816022
284.488021	7999.890045	10.392077	-0.058053	4.816024
284.632257	7999.892661	10.397082	-0.058080	4.816024
284.431069	7999.895420	10.402087	-0.058042	4.816026
284.579306	7999.788063	10.407091	-0.058070	4.815994
284.712465	7999.924030	10.412096	-0.058095	4.816033
284.525512	7999.878968	10.417101	-0.058060	4.816020
284.611750	7999.865574	10.422106	-0.058076	4.816016
284.629187	7999.987689	10.427111	-0.058079	4.816052
284.542650	7999.861113	10.432115	-0.058063	4.816015
284.597638	7999.875999	10.437120	-0.058073	4.816019
284.690855	7999.881964	10.442125	-0.058091	4.816020
284.671857	7999.792940	10.447130	-0.058087	4.815995
284.459729	7999.941873	10.452135	-0.058048	4.816039
284.489250	7999.762915	10.457139	-0.058053	4.815987
284.641653	7999.902436	10.462144	-0.058081	4.816027
284.490421	7999.861228	10.467149	-0.058053	4.816015
284.539429	7999.810832	10.472154	-0.058062	4.816000
284.659562	7999.941221	10.477159	-0.058085	4.816038
284.505280	7999.895684	10.482163	-0.058056	4.816025
284.631011	7999.938564	10.487168	-0.058079	4.816037
284.553178	7999.899756	10.492173	-0.058065	4.816026
284.589421	7999.888660	10.497178	-0.058072	4.816023
284.617247	7999.872070	10.502183	-0.058077	4.816018
284.489338	7999.888979	10.507187	-0.058053	4.816024
284.419349	7999.832151	10.512192	-0.058040	4.816007
284.401129	7999.857462	10.517197	-0.058036	4.816015
284.534180	7999.889790	10.522202	-0.058061	4.816024
284.722199	7999.778881	10.527207	-0.058096	4.815990
284.827541	7999.898317	10.532211	-0.058116	4.816025
284.829646	7999.872712	10.537216	-0.058116	4.816017
284.548890	7999.876164	10.542221	-0.058064	4.816020
284.744413	7999.799580	10.547226	-0.058100	4.815996
284.583979	7999.939836	10.552231	-0.058070	4.816038
284.523200	7999.863943	10.557235	-0.058059	4.816016
284.631607	7999.893688	10.562240	-0.058079	4.816024
284.436575	7999.791854	10.567245	-0.058043	4.815995
284.407289	7999.872521	10.572250	-0.058037	4.816019
284.633446	7999.927908	10.577255	-0.058080	4.816034
284.571990	7999.768667	10.582259	-0.058068	4.815988
284.735814	7999.856042	10.587264	-0.058099	4.816013
284.564704	7999.948026	10.592269	-0.058067	4.816040
284.720530	7999.865379	10.597274	-0.058096	4.816015
284.677636	7999.806906	10.602279	-0.058088	4.815999
284.533115	7999.876935	10.607283	-0.058061	4.816020
284.764501	7999.868311	10.612288	-0.058104	4.816016
284.655995	7999.835357	10.617293	-0.058084	4.816007
284.751424	7999.815720	10.622298	-0.058101	4.816001
284.708572	7999.902551	10.627303	-0.058094	4.816026
284.749833	7999.864836	10.632307	-0.058101	4.816015
284.762349	7999.858652	10.637312	-0.058103	4.816013
284.565472	7999.827300	10.642317	-0.058067	4.816005
284.963127	7999.851609	10.647322	-0.058141	4.816010
284.899112	7999.899594	10.652327	-0.058129	4.816025
284.858119	7999.851838	10.657331	-0.058121	4.816011
285.019287	7999.860104	10.662336	-0.058151	4.816012
284.828858	7999.939985	10.667341	-0.058116	4.816037
284.601240	7999.873885	10.672346	-0.058073	4.816019
284.716963	7999.819358	10.677351	-0.058095	4.816002
284.974475	7999.883861	10.682355	-0.058143	4.816020
284.851400	7999.836753	10.687360	-0.058120	4.816006
284.900506	7999.840849	10.692365	-0.058129	4.816007
284.896402	7999.874963	10.697370	-0.058128	4.816017
284.932136	7999.904458	10.702375	-0.058135	4.816026
284.785878	7999.879366	10.707379	-0.058108	4.816019
284.705676	7999.798847	10.712384	-0.058093	4.815996
284.899541	7999.858990	10.717389	-0.058129	4.816013
284.855484	7999.968237	10.722394	-0.058121	4.816045
285.028207	7999.893375	10.727399	-0.058153	4.816022
285.002832	7999.882230	10.732403	-0.058148	4.816019
284.930770	7999.811474	10.737408	-0.058135	4.815999
285.041913	7999.793190	10.742413	-0.058155	4.815993
285.129498	7999.873841	10.747418	-0.058172	4.816016
285.116105	7999.919540	10.752423	-0.058169	4.816029
284.987866	7999.776180	10.757427	-0.058145	4.815988
285.033649	7999.898810	10.762432	-0.058154	4.816024
285.070146	7999.874898	10.767437	-0.058161	4.816016
284.966896	7999.905076	10.772442	-0.058141	4.816026
284.836366	7999.809754	10.777447	-0.058117	4.815999
284.982115	7999.964114	10.782451	-0.058144	4.816043
285.046463	7999.864848	10.787456	-0.058156	4.816014
284.878346	7999.879960	10.792461	-0.058125	4.816019
285.060766	7999.759332	10.797466	-0.058159	4.815983
285.014740	7999.899528	10.802471	-0.058150	4.816024
284.927350	7999.986621	10.807475	-0.058134	4.816050
285.063840	7999.919649	10.812480	-0.058159	4.816030
285.128300	7999.795812	10.817485	-0.058171	4.815993
285.115945	7999.897087	10.822490	-0.058169	4.816023
284.869645	7999.824238	10.827495	-0.058123	4.816003
284.971481	7999.890190	10.832499	-0.058142	4.816021
284.878488	7999.923760	10.837504	-0.058125	4.816032
284.882157	7999.877883	10.842509	-0.058125	4.816018
284.992484	7999.853174	10.847514	-0.058146	4.816010
285.107369	7999.918295	10.852519	-0.058167	4.816029
284.873292	7999.878788	10.857523	-0.058124	4.816019
284.870364	7999.899034	10.862528	-0.058123	4.816025
284.853308	7999.891244	10.867533	-0.058120	4.816022
285.047307	7999.890490	10.872538	-0.058156	4.816021
284.912691	7999.832489	10.877543	-0.058131	4.816005
285.088603	7999.849569	10.882547	-0.058164	4.816009
284.915696	7999.856047	10.887552	-0.058132	4.816012
285.094688	7999.943700	10.892557	-0.058165	4.816036
285.105449	7999.780425	10.897562	-0.058167	4.815989
285.248253	7999.922979	10.902567	-0.058194	4.816030
285.073163	7999.924074	10.907571	-0.058161	4.816031
285.038559	7999.825150	10.912576	-0.058154	4.816002
285.130122	7999.899464	10.917581	-0.058171	4.816023
285.228308	7999.795471	10.922586	-0.058190	4.815992
285.201484	7999.883662	10.927591	-0.058185	4.816018
285.139639	7999.857965	10.932595	-0.058173	4.816011
285.163240	7999.828477	10.937600	-0.058178	4.816002
285.120972	7999.928141	10.942605	-0.058170	4.816032
285.037163	7999.793066	10.947610	-0.058154	4.815993
284.984116	7999.888261	10.952615	-0.058144	4.816021
284.999016	7999.867162	10.957619	-0.058147	4.816015
284.887079	7999.811708	10.962624	-0.058126	4.815999
284.867351	7999.803871	10.967629	-0.058122	4.815997
285.010192	7999.845993	10.972634	-0.058149	4.816008
285.108372	7999.901195	10.977639	-0.058167	4.816024
284.982700	7999.877545	10.982643	-0.058144	4.816018
285.064177	7999.891844	10.987648	-0.058159	4.816021
285.156638	7999.874289	10.992653	-0.058176	4.816016
285.086852	7999.879432	10.997658	-0.058163	4.816018
285.269893	7999.903054	11.002663	-0.058197	4.816024
285.205159	7999.909357	11.007667	-0.058185	4.816026
285.317844	7999.817379	11.012672	-0.058206	4.815998
285.061216	7999.955890	11.017677	-0.058158	4.816040
285.064623	7999.865135	11.022682	-0.058159	4.816014
284.961174	7999.847230	11.027687	-0.058140	4.816009
285.041034	7999.889279	11.032691	-0.058155	4.816021
285.222421	7999.854106	11.037696	-0.058188	4.816010
285.221899	7999.942776	11.042701	-0.058188	4.816035
285.165102	7999.792164	11.047706	-0.058178	4.815992
285.253443	7999.866419	11.052711	-0.058194	4.816013
285.117117	7999.892792	11.057715	-0.058169	4.816021
285.277854	7999.889298	11.062720	-0.058199	4.816020
285.100407	7999.793123	11.067725	-0.058166	4.815992
285.094484	7999.875284	11.072730	-0.058165	4.816016
285.166411	7999.886204	11.077735	-0.058178	4.816019
285.181487	7999.882203	11.082739	-0.058181	4.816018
285.269947	7999.832523	11.087744	-0.058197	4.816003
285.142659	7999.911412	11.092749	-0.058173	4.816027
285.088546	7999.989493	11.097754	-0.058163	4.816050
285.300486	7999.960218	11.102759	-0.058203	4.816040
285.179942	7999.834091	11.107763	-0.058180	4.816004
285.244121	7999.835255	11.112768	-0.058192	4.816004
285.183523	7999.924971	11.117773	-0.058181	4.816030
285.229863	7999.970685	11.122778	-0.058190	4.816044
285.278740	7999.845496	11.127783	-0.058199	4.816007
285.087307	7999.957411	11.132787	-0.058163	4.816040
285.310175	7999.852475	11.137792	-0.058205	4.816009
285.121134	7999.917423	11.142797	-0.058169	4.816029
285.003064	7999.877885	11.147802	-0.058147	4.816018
285.171985	7999.863854	11.152807	-0.058179	4.816013
285.205283	7999.975575	11.157811	-0.058185	4.816045
285.464212	7999.837103	11.162816	-0.058233	4.816003
285.423444	7999.919700	11.167821	-0.058226	4.816028
285.316215	7999.881426	11.172826	-0.058206	4.816017
285.150774	7999.805770	11.177831	-0.058175	4.815996
285.252748	7999.869588	11.182835	-0.058194	4.816014
285.179631	7999.845823	11.187840	-0.058180	4.816007
285.264888	7999.977719	11.192845	-0.058196	4.816045
285.277415	7999.751438	11.197850	-0.058198	4.815979
285.396731	7999.867924	11.202855	-0.058221	4.816013
285.281419	7999.856214	11.207859	-0.058199	4.816010
285.428684	7999.974278	11.212864	-0.058227	4.816044
285.272620	7999.996018	11.217869	-0.058197	4.816051
285.392685	7999.794125	11.222874	-0.058220	4.815991
285.452486	7999.900984	11.227879	-0.058231	4.816022
285.332885	7999.887060	11.232883	-0.058209	4.816019
285.376874	7999.803451	11.237888	-0.058217	4.815994
285.185648	7999.998708	11.242893	-0.058181	4.816052
285.044565	7999.879688	11.247898	-0.058155	4.816018
285.318270	7999.801317	11.252903	-0.058206	4.815994
285.132032	7999.896231	11.257907	-0.058171	4.816022
285.180643	7999.921687	11.262912	-0.058180	4.816030
285.188328	7999.956015	11.267917	-0.058182	4.816040
285.223070	7999.797449	11.272922	-0.058188	4.815993
285.223925	7999.911785	11.277927	-0.058188	4.816026
285.135681	7999.965741	11.282931	-0.058172	4.816043
285.438591	7999.866531	11.287936	-0.058228	4.816012
285.442335	7999.881557	11.292941	-0.058229	4.816016
285.409950	7999.874557	11.297946	-0.058223	4.816015
285.332376	7999.889175	11.302951	-0.058208	4.816019
285.328399	7999.857049	11.307955	-0.058208	4.816010
285.325070	7999.894383	11.312960	-0.058207	4.816021
285.246942	7999.910059	11.317965	-0.058192	4.816026
285.351491	7999.777333	11.322970	-0.058212	4.815986
285.559588	7999.977701	11.327975	-0.058251	4.816044
285.349829	7999.869186	11.332979	-0.058212	4.816013
285.358266	7999.875749	11.337984	-0.058213	4.816015
285.321446	7999.930638	11.342989	-0.058206	4.816031
285.464871	7999.858450	11.347994	-0.058233	4.816010
285.552500	7999.896366	11.352999	-0.058249	4.816020
285.491269	7999.859996	11.358003	-0.058238	4.816010
285.475362	7999.898170	11.363008	-0.058235	4.816021
285.243336	7999.834126	11.368013	-0.058192	4.816004
285.354367	7999.892767	11.373018	-0.058212	4.816020
285.635178	7999.834825	11.378023	-0.058265	4.816002
285.612998	7999.883569	11.383027	-0.058260	4.816016
285.671774	7999.924168	11.388032	-0.058271	4.816028
285.473040	7999.884232	11.393037	-0.058234	4.816017
285.461066	7999.876535	11.398042	-0.058232	4.816015
285.409502	7999.877735	11.403047	-0.058223	4.816015
285.411442	7999.846785	11.408051	-0.058223	4.816006
285.457396	7999.845481	11.413056	-0.058231	4.816006
285.487700	7999.906931	11.418061	-0.058237	4.816024
285.679880	7999.886913	11.423066	-0.058273	4.816017
285.666330	7999.842860	11.428071	-0.058270	4.816004
285.472447	7999.869256	11.433075	-0.058234	4.816013
285.535100	7999.850092	11.438080	-0.058246	4.816007
285.734271	7999.808832	11.443085	-0.058283	4.815994
285.562134	7999.924303	11.448090	-0.058251	4.816028
285.560785	7999.920004	11.453095	-0.058251	4.816027
285.478199	7999.809524	11.458099	-0.058235	4.815995
285.611729	7999.921996	11.463104	-0.058260	4.816027
285.566721	7999.898740	11.468109	-0.058252	4.816021
285.723697	7999.899452	11.473114	-0.058281	4.816020
285.676211	7999.798156	11.478119	-0.058272	4.815991
285.514965	7999.856129	11.483123	-0.058242	4.816009
285.636976	7999.943818	11.488128	-0.058265	4.816034
285.529762	7999.901270	11.493133	-0.058245	4.816022
285.764651	7999.872411	11.498138	-0.058289	4.816012
285.728063	7999.876020	11.503143	-0.058282	4.816013
285.543652	7999.980584	11.508147	-0.058247	4.816045
285.477843	7999.769975	11.513152	-0.058235	4.815984
285.556704	7999.857949	11.518157	-0.058250	4.816009
285.547170	7999.849227	11.523162	-0.058248	4.816006
285.804708	7999.928692	11.528167	-0.058296	4.816028
285.671784	7999.963674	11.533171	-0.058271	4.816039
285.675554	7999.836597	11.538176	-0.058272	4.816002
285.870032	7999.893548	11.543181	-0.058308	4.816018
285.742808	7999.872006	11.548186	-0.058284	4.816012
285.733670	7999.907098	11.553191	-0.058283	4.816022
285.769711	7999.901340	11.558195	-0.058289	4.816020
285.779166	7999.781846	11.563200	-0.058291	4.815985
285.707056	7999.949350	11.568205	-0.058278	4.816035
285.567238	7999.865609	11.573210	-0.058252	4.816011
285.766166	7999.938668	11.578215	-0.058289	4.816031
285.723819	7999.873792	11.583219	-0.058281	4.816013
285.680338	7999.870865	11.588224	-0.058273	4.816012
285.756972	7999.928882	11.593229	-0.058287	4.816029
285.610774	7999.886695	11.598234	-0.058260	4.816017
285.564625	7999.964921	11.603239	-0.058251	4.816040
285.684720	8000.352814	11.608243	-0.058274	4.816153
285.981652	7999.873124	11.613248	-0.058329	4.816011
285.676426	7999.989385	11.618253	-0.058272	4.816047
285.785544	7999.875973	11.623258	-0.058292	4.816013
285.835322	7999.792469	11.628263	-0.058301	4.815988
285.750118	7999.936230	11.633267	-0.058286	4.816031
285.816655	7999.787854	11.638272	-0.058298	4.815987
286.032338	8000.066361	11.643277	-0.058338	4.816067
285.998942	7999.884116	11.648282	-0.058332	4.816014
285.947610	7999.819077	11.653287	-0.058322	4.815995
285.825105	7999.931176	11.658291	-0.058300	4.816029
285.933283	7999.809199	11.663296	-0.058320	4.815993
285.840844	7999.879106	11.668301	-0.058302	4.816014
285.813665	7999.896775	11.673306	-0.058297	4.816019
285.868148	7999.868915	11.678311	-0.058307	4.816010
285.780541	7999.950663	11.683315	-0.058291	4.816035
285.623220	7999.957422	11.688320	-0.058262	4.816038
285.868771	7999.913798	11.693325	-0.058308	4.816024
285.903794	7999.936871	11.698330	-0.058314	4.816030
285.843401	7999.863119	11.703335	-0.058303	4.816009
285.773068	7999.971891	11.708339	-0.058290	4.816041
286.048782	7999.798465	11.713344	-0.058341	4.815989
286.037890	7999.915796	11.718349	-0.058339	4.816023
285.830413	7999.858606	11.723354	-0.058300	4.816008
285.938068	7999.848806	11.728359	-0.058320	4.816004
285.927289	8000.061232	11.733363	-0.058318	4.816066
285.912938	7999.864375	11.738368	-0.058316	4.816009
285.990246	7999.887146	11.743373	-0.058330	4.816015
286.011905	7999.926003	11.748378	-0.058334	4.816026
285.911274	7999.836562	11.753383	-0.058315	4.816001
285.771954	7999.887455	11.758387	-0.058289	4.816016
285.873497	7999.834806	11.763392	-0.058308	4.816000
285.814317	7999.893564	11.768397	-0.058297	4.816018
285.613746	7999.839706	11.773402	-0.058260	4.816003
285.767170	7999.867064	11.778407	-0.058288	4.816010
285.715658	7999.853307	11.783411	-0.058279	4.816007
285.861972	7999.958533	11.788416	-0.058306	4.816037
285.615047	7999.951912	11.793421	-0.058260	4.816036
285.871622	7999.789891	11.798426	-0.058308	4.815987
285.898450	7999.908975	11.803431	-0.058313	4.816022
285.701740	7999.814586	11.808435	-0.058276	4.815995
285.961385	7999.935758	11.813440	-0.058325	4.816030
285.973332	7999.807761	11.818445	-0.058327	4.815992
285.657978	7999.898195	11.823450	-0.058268	4.816020
285.928588	7999.940502	11.828455	-0.058318	4.816031
286.006753	7999.838281	11.833459	-0.058333	4.816001
285.945652	7999.846787	11.838464	-0.058322	4.816004
285.975953	7999.946702	11.843469	-0.058327	4.816033
285.802929	7999.806799	11.848474	-0.058295	4.815993
285.721204	7999.876900	11.853479	-0.058280	4.816014
285.801402	7999.927504	11.858483	-0.058295	4.816028
286.008667	7999.819078	11.863488	-0.058333	4.815995
286.239652	7999.864940	11.868493	-0.058376	4.816007
285.989323	7999.925570	11.873498	-0.058330	4.816026
286.080425	7999.832131	11.878503	-0.058347	4.815999
285.868331	7999.978931	11.883507	-0.058307	4.816043
285.911748	7999.782056	11.888512	-0.058315	4.815985
285.876246	7999.947020	11.893517	-0.058309	4.816033
285.892425	7999.882137	11.898522	-0.058312	4.816014
285.961365	7999.810733	11.903527	-0.058324	4.815993
285.829460	7999.973947	11.908531	-0.058300	4.816041
285.705764	7999.812503	11.913536	-0.058277	4.815995
286.003450	7999.873464	11.918541	-0.058332	4.816011
285.808062	7999.910517	11.923546	-0.058296	4.816023
285.835947	7999.794562	11.928551	-0.058301	4.815989
285.722222	7999.905752	11.933555	-0.058280	4.816022
286.115593	7999.844511	11.938560	-0.058353	4.816002
285.815403	7999.868978	11.943565	-0.058297	4.816011
285.791102	7999.902726	11.948570	-0.058293	4.816021
285.915054	7999.817363	11.953575	-0.058316	4.815995
285.926493	7999.887018	11.958579	-0.058318	4.816015
286.013905	7999.904631	11.963584	-0.058334	4.816020
286.084960	7999.895235	11.968589	-0.058347	4.816017
286.003924	7999.813630	11.973594	-0.058332	4.815994
286.059785	7999.946062	11.978599	-0.058343	4.816032
286.127965	7999.822290	11.983603	-0.058355	4.815995
286.130432	7999.835156	11.988608	-0.058356	4.815999
286.151583	7999.966959	11.993613	-0.058360	4.816038
286.087125	7999.826888	11.998618	-0.058348	4.815997
286.274916	7999.915773	12.003623	-0.058383	4.816022
285.993415	7999.817706	12.008627	-0.058330	4.815995
286.068890	7999.907757	12.013632	-0.058344	4.816021
286.191320	7999.920663	12.018637	-0.058367	4.816024
286.104378	7999.812239	12.023642	-0.058351	4.815993
285.849217	7999.875987	12.028647	-0.058303	4.816013
285.819399	7999.876513	12.033651	-0.058298	4.816013
286.086030	7999.857846	12.038656	-0.058347	4.816006
286.049192	7999.910599	12.043661	-0.058340	4.816022
286.079313	7999.964568	12.048666	-0.058346	4.816037
286.069060	7999.816934	12.053671	-0.058344	4.815994
285.980097	7999.844167	12.058675	-0.058328	4.816003
286.021617	7999.882315	12.063680	-0.058335	4.816014
285.991130	7999.924499	12.068685	-0.058330	4.816026
286.000371	7999.791110	12.073690	-0.058331	4.815987
285.942796	7999.915072	12.078695	-0.058321	4.816024
285.962917	7999.891930	12.083699	-0.058324	4.816017
285.986679	7999.876334	12.088704	-0.058329	4.816012
285.932416	7999.907402	12.093709	-0.058319	4.816021
285.902591	7999.767962	12.098714	-0.058313	4.815981
286.212982	7999.844112	12.103719	-0.058371	4.816001
286.105660	7999.914818	12.108723	-0.058351	4.816023
286.082132	7999.787244	12.113728	-0.058346	4.815985
285.829797	7999.934382	12.118733	-0.058300	4.816030
285.917381	7999.910329	12.123738	-0.058316	4.816022
286.043164	7999.826067	12.128743	-0.058339	4.815997
286.002430	7999.928966	12.133747	-0.058332	4.816027
286.083357	7999.898381	12.138752	-0.058347	4.816018
286.153989	7999.845171	12.143757	-0.058360	4.816002
286.086859	7999.877073	12.148762	-0.058347	4.816012
286.189339	7999.811621	12.153767	-0.058366	4.815992
286.029713	7999.975400	12.158771	-0.058337	4.816041
286.075599	7999.776432	12.163776	-0.058345	4.815982
286.358469	7999.946109	12.168781	-0.058398	4.816030
286.310931	7999.784976	12.173786	-0.058389	4.815984
286.303564	7999.913056	12.178791	-0.058388	4.816021
286.077354	7999.804240	12.183795	-0.058345	4.815990
286.231295	7999.901057	12.188800	-0.058374	4.816018
286.152538	7999.834451	12.193805	-0.058359	4.815999
286.087666	7999.970034	12.198810	-0.058347	4.816039
286.281021	7999.868835	12.203815	-0.058383	4.816008
286.263512	7999.893091	12.208819	-0.058380	4.816015
286.130595	7999.918457	12.213824	-0.058355	4.816024
286.231398	7999.882890	12.218829	-0.058374	4.816013
286.210607	7999.864348	12.223834	-0.058370	4.816007
286.327955	7999.922037	12.228839	-0.058392	4.816024
286.123016	7999.880920	12.233843	-0.058354	4.816013
286.279741	7999.803630	12.238848	-0.058383	4.815989
286.327106	7999.960484	12.243853	-0.058392	4.816035
286.200282	7999.891936	12.248858	-0.058368	4.816015
286.316668	7999.812845	12.253863	-0.058390	4.815992
286.275014	8000.021506	12.258867	-0.058382	4.816053
286.097009	7999.890058	12.263872	-0.058349	4.816015
286.147383	7999.876013	12.268877	-0.058358	4.816011
286.248668	7999.889604	12.273882	-0.058377	4.816015
286.119404	7999.844519	12.278887	-0.058353	4.816002
286.118886	7999.902205	12.283891	-0.058353	4.816019
286.170936	7999.880711	12.288896	-0.058363	4.816012
286.138630	7999.933546	12.293901	-0.058357	4.816028
285.993861	7999.789882	12.298906	-0.058330	4.815987
286.352177	7999.856219	12.303911	-0.058396	4.816004
286.355229	7999.926792	12.308915	-0.058397	4.816025
286.242446	7999.843541	12.313920	-0.058376	4.816001
286.304100	7999.847864	12.318925	-0.058387	4.816002
286.291572	7999.871142	12.323930	-0.058385	4.816009
286.186514	7999.946163	12.328935	-0.058366	4.816031
286.094999	7999.894283	12.333939	-0.058348	4.816017
286.270825	7999.786355	12.338944	-0.058381	4.815984
286.349200	7999.953388	12.343949	-0.058396	4.816033
286.149194	7999.872826	12.348954	-0.058359	4.816010
286.185077	7999.867066	12.353959	-0.058365	4.816008
286.254380	7999.864050	12.358963	-0.058378	4.816007
286.234963	7999.909640	12.363968	-0.058374	4.816020
286.290662	7999.871117	12.368973	-0.058385	4.816009
286.217860	7999.899711	12.373978	-0.058371	4.816018
286.309156	7999.832987	12.378983	-0.058388	4.815998
286.193983	7999.908892	12.383987	-0.058367	4.816020
286.250172	7999.812682	12.388992	-0.058377	4.815992
286.353812	7999.924614	12.393997	-0.058397	4.816024
286.299612	7999.862727	12.399002	-0.058386	4.816006
286.345372	7999.834708	12.404007	-0.058395	4.815998
286.249715	7999.910968	12.409011	-0.058377	4.816021
286.131592	7999.886385	12.414016	-0.058355	4.816014
286.189836	7999.944070	12.419021	-0.058366	4.816031
286.072574	7999.965446	12.424026	-0.058344	4.816038
286.205913	7999.893074	12.429031	-0.058369	4.816016
286.198213	7999.854469	12.434035	-0.058367	4.816005
286.253785	7999.867230	12.439040	-0.058378	4.816008
286.244951	7999.927970	12.444045	-0.058376	4.816026
286.157927	7999.932800	12.449050	-0.058360	4.816028
286.188010	7999.855348	12.454055	-0.058366	4.816005
286.245019	7999.906600	12.459059	-0.058376	4.816020
286.318772	7999.874816	12.464064	-0.058390	4.816010
286.282810	7999.931859	12.469069	-0.058383	4.816027
286.367168	7999.878898	12.474074	-0.058399	4.816011
286.456459	7999.846327	12.479079	-0.058415	4.816001
286.248017	7999.803009	12.484083	-0.058377	4.815989
286.302456	7999.885199	12.489088	-0.058387	4.816013
286.543022	7999.888498	12.494093	-0.058432	4.816013
286.284039	7999.794045	12.499098	-0.058383	4.815986
286.349039	7999.920233	12.504103	-0.058395	4.816023
286.252015	7999.885348	12.509107	-0.058377	4.816013
286.224375	7999.802575	12.514112	-0.058372	4.815989
286.161333	7999.954218	12.519117	-0.058361	4.816034
286.308272	7999.873546	12.524122	-0.058388	4.816010
286.451805	7999.852645	12.529127	-0.058415	4.816003
286.385596	7999.861058	12.534131	-0.058402	4.816005
286.563660	7999.884591	12.539136	-0.058435	4.816011
286.541814	7999.860687	12.544141	-0.058431	4.816005
286.321004	7999.870567	12.549146	-0.058390	4.816009
286.446993	7999.899565	12.554151	-0.058414	4.816016
286.246893	7999.883109	12.559155	-0.058376	4.816013
286.293959	7999.788871	12.564160	-0.058385	4.815985
286.344565	7999.947920	12.569165	-0.058395	4.816031
286.515829	7999.885853	12.574170	-0.058426	4.816012
286.605244	7999.870380	12.579175	-0.058443	4.816007
286.289942	7999.856107	12.584179	-0.058384	4.816005
286.243168	7999.798628	12.589184	-0.058376	4.815988
286.456878	7999.922175	12.594189	-0.058415	4.816023
286.266748	7999.879189	12.599194	-0.058380	4.816011
286.227810	7999.828264	12.604199	-0.058373	4.815997
286.449226	7999.891048	12.609203	-0.058414	4.816014
286.333199	7999.896419	12.614208	-0.058392	4.816016
286.245412	7999.909783	12.619213	-0.058376	4.816020
286.225306	7999.905143	12.624218	-0.058372	4.816019
286.377637	7999.840595	12.629223	-0.058401	4.816000
286.263377	7999.940023	12.634227	-0.058379	4.816029
286.509054	7999.919909	12.639232	-0.058425	4.816022
286.500875	7999.860994	12.644237	-0.058423	4.816005
286.290368	7999.861445	12.649242	-0.058384	4.816006
286.220986	7999.923223	12.654247	-0.058371	4.816025
286.334018	7999.836592	12.659251	-0.058392	4.815999
286.356867	7999.909661	12.664256	-0.058397	4.816020
286.287174	7999.895574	12.669261	-0.058384	4.816016
286.281428	7999.875168	12.674266	-0.058383	4.816010
286.432311	7999.790293	12.679271	-0.058411	4.815985
286.112234	7999.972529	12.684275	-0.058351	4.816040
286.249203	7999.880991	12.689280	-0.058377	4.816012
286.452959	7999.907127	12.694285	-0.058414	4.816019
286.217239	8000.000076	12.699290	-0.058371	4.816047
286.274907	7999.878249	12.704295	-0.058381	4.816011
286.474153	7999.905372	12.709299	-0.058418	4.816018
286.620586	7999.789431	12.714304	-0.058446	4.815983
286.452267	7999.937027	12.719309	-0.058414	4.816027
286.563185	7999.825783	12.724314	-0.058435	4.815994
286.691004	7999.878321	12.729319	-0.058459	4.816009
286.428025	7999.922694	12.734323	-0.058410	4.816023
286.376146	7999.804221	12.739328	-0.058400	4.815989
286.440378	7999.947491	12.744333	-0.058412	4.816030
286.269091	7999.857835	12.749338	-0.058380	4.816005
286.498276	7999.931445	12.754343	-0.058423	4.816025
286.486074	7999.914127	12.759347	-0.058421	4.816020
286.357992	7999.890431	12.764352	-0.058397	4.816014
286.378031	7999.905753	12.769357	-0.058400	4.816019
286.368826	7999.892763	12.774362	-0.058399	4.816015
286.512232	7999.795999	12.779367	-0.058425	4.815986
286.384615	7999.968909	12.784371	-0.058402	4.816037
286.374093	7999.913157	12.789376	-0.058400	4.816021
286.532637	7999.914966	12.794381	-0.058429	4.816020
286.326100	7999.918694	12.799386	-0.058391	4.816023
286.495601	7999.873690	12.804391	-0.058422	4.816009
286.295449	7999.894630	12.809395	-0.058385	4.816016
286.486881	7999.871393	12.814400	-0.058421	4.816008
286.379869	7999.883339	12.819405	-0.058401	4.816012
286.180234	7999.891467	12.824410	-0.058363	4.816015
286.335900	7999.862238	12.829415	-0.058392	4.816006
286.258112	7999.952713	12.834419	-0.058378	4.816033
286.145273	7999.900446	12.839424	-0.058357	4.816018
286.240111	7999.929946	12.844429	-0.058375	4.816026
286.218403	7999.881471	12.849434	-0.058370	4.816012
286.339380	7999.807806	12.854439	-0.058393	4.815990
286.107942	7999.912586	12.859443	-0.058350	4.816022
286.280846	7999.898629	12.864448	-0.058382	4.816017
286.467779	7999.850736	12.869453	-0.058417	4.816002
286.137014	7999.913111	12.874458	-0.058355	4.816022
286.429778	7999.830812	12.879463	-0.058410	4.815996
286.356841	7999.875430	12.884467	-0.058396	4.816010
286.346035	7999.885918	12.889472	-0.058394	4.816013
286.369318	7999.947242	12.894477	-0.058399	4.816031
286.376434	7999.874715	12.899482	-0.058400	4.816010
286.306078	7999.780481	12.904487	-0.058387	4.815982
286.275397	7999.975451	12.909491	-0.058381	4.816040
286.305677	7999.886249	12.914496	-0.058387	4.816013
286.543526	7999.827527	12.919501	-0.058431	4.815995
286.313465	7999.928058	12.924506	-0.058388	4.816025
286.351373	7999.837927	12.929511	-0.058395	4.815999
286.418292	7999.834867	12.934515	-0.058408	4.815998
286.445385	7999.863138	12.939520	-0.058413	4.816006
286.449997	7999.951903	12.944525	-0.058413	4.816032
286.504435	7999.809717	12.949530	-0.058424	4.815990
286.497184	7999.889719	12.954535	-0.058422	4.816013
286.350537	7999.900945	12.959539	-0.058395	4.816017
286.412879	7999.835832	12.964544	-0.058406	4.815998
286.687579	7999.884625	12.969549	-0.058458	4.816011
286.497887	7999.888659	12.974554	-0.058422	4.816013
286.743827	7999.883508	12.979559	-0.058468	4.816010
286.522190	7999.964960	12.984563	-0.058427	4.816035
286.550012	7999.882124	12.989568	-0.058432	4.816011
286.542824	7999.914046	12.994573	-0.058431	4.816020
286.474000	7999.854030	12.999578	-0.058418	4.816003
286.642828	7999.874190	13.004583	-0.058449	4.816008
286.366002	7999.922586	13.009587	-0.058398	4.816024
286.468660	7999.813329	13.014592	-0.058417	4.815991
286.668558	7999.878929	13.019597	-0.058454	4.816009
286.268042	7999.899435	13.024602	-0.058379	4.816017
286.414244	7999.857214	13.029607	-0.058407	4.816004
286.511012	7999.971158	13.034611	-0.058425	4.816037
286.434063	7999.882146	13.039616	-0.058410	4.816011
286.542620	7999.884116	13.044621	-0.058430	4.816011
286.541682	7999.859524	13.049626	-0.058430	4.816004
286.645438	7999.915899	13.054631	-0.058450	4.816020
286.610089	7999.917393	13.059635	-0.058443	4.816021
286.538023	7999.907536	13.064640	-0.058430	4.816018
286.543852	7999.865970	13.069645	-0.058431	4.816006
286.469968	7999.926599	13.074650	-0.058417	4.816024
286.553750	7999.866148	13.079655	-0.058432	4.816006
286.460233	7999.884750	13.084659	-0.058415	4.816012
286.680971	7999.871662	13.089664	-0.058456	4.816007
286.614849	7999.922815	13.094669	-0.058444	4.816022
286.692711	7999.929571	13.099674	-0.058458	4.816024
286.756962	7999.858081	13.104679	-0.058470	4.816003
286.624902	7999.960391	13.109683	-0.058446	4.816033
286.527224	7999.910536	13.114688	-0.058428	4.816019
286.687583	7999.887803	13.119693	-0.058457	4.816012
286.580863	7999.823894	13.124698	-0.058437	4.815994
286.578597	7999.894370	13.129703	-0.058437	4.816014
286.532953	7999.918115	13.134707	-0.058429	4.816021
286.645398	7999.887034	13.139712	-0.058449	4.816012
286.591427	7999.834767	13.144717	-0.058439	4.815997
286.621528	7999.923995	13.149722	-0.058445	4.816023
286.649276	7999.855048	13.154727	-0.058450	4.816002
286.569468	7999.886720	13.159731	-0.058435	4.816012
286.526181	7999.813278	13.164736	-0.058427	4.815991
286.647552	7999.919121	13.169741	-0.058450	4.816021
286.466591	7999.883781	13.174746	-0.058416	4.816012
286.441911	7999.801060	13.179751	-0.058411	4.815988
286.558398	7999.939938	13.184755	-0.058433	4.816028
286.603413	7999.795443	13.189760	-0.058441	4.815985
286.506139	7999.944329	13.194765	-0.058423	4.816029
286.506335	7999.887703	13.199770	-0.058423	4.816013
286.623035	7999.816097	13.204775	-0.058445	4.815991
286.593982	7999.972633	13.209779	-0.058440	4.816037
286.550751	7999.845768	13.214784	-0.058432	4.816000
286.679397	7999.886568	13.219789	-0.058456	4.816011
286.573272	7999.922036	13.224794	-0.058436	4.816022
286.635012	7999.841953	13.229799	-0.058447	4.815999
286.742031	7999.968907	13.234803	-0.058467	4.816035
286.637477	7999.817422	13.239808	-0.058448	4.815991
286.395718	7999.929493	13.244813	-0.058403	4.816025
286.336635	7999.900640	13.249818	-0.058392	4.816017
286.523826	7999.846341	13.254823	-0.058427	4.816000
286.469358	7999.928691	13.259827	-0.058416	4.816025
286.500222	7999.799967	13.264832	-0.058422	4.815987
286.685023	7999.897346	13.269837	-0.058457	4.816015
286.547260	7999.900186	13.274842	-0.058431	4.816016
286.546760	7999.840342	13.279847	-0.058431	4.815999
286.462719	7999.876211	13.284851	-0.058415	4.816010
286.673136	7999.892852	13.289856	-0.058454	4.816013
286.531474	7999.991784	13.294861	-0.058428	4.816043
286.653065	7999.832652	13.299866	-0.058451	4.815996
286.657865	7999.867998	13.304871	-0.058451	4.816006
286.503029	7999.958142	13.309875	-0.058423	4.816033
286.627562	7999.819365	13.314880	-0.058446	4.815992
286.740120	7999.868420	13.319885	-0.058467	4.816006
286.621462	7999.981659	13.324890	-0.058445	4.816040
286.609199	7999.801933	13.329895	-0.058442	4.815987
286.506929	7999.993467	13.334899	-0.058423	4.816044
286.439104	7999.782816	13.339904	-0.058411	4.815982
286.570789	7999.890984	13.344909	-0.058435	4.816013
286.307050	7999.957781	13.349914	-0.058386	4.816034
286.515584	7999.868610	13.354919	-0.058425	4.816007
286.627086	7999.874908	13.359923	-0.058446	4.816008
286.549516	7999.933333	13.364928	-0.058431	4.816026
286.720477	7999.838137	13.369933	-0.058463	4.815997
286.702676	7999.938249	13.374938	-0.058460	4.816026
286.520532	7999.844121	13.379943	-0.058426	4.816000
286.490415	7999.900202	13.384947	-0.058420	4.816016
286.510899	7999.885614	13.389952	-0.058424	4.816012
286.652935	7999.895672	13.394957	-0.058450	4.816014
286.599054	7999.929952	13.399962	-0.058440	4.816025
286.652699	7999.842242	13.404967	-0.058450	4.815999
286.740459	7999.865204	13.409971	-0.058467	4.816005
286.665176	7999.891617	13.414976	-0.058453	4.816013
286.619101	7999.866204	13.419981	-0.058444	4.816006
286.774011	7999.910687	13.424986	-0.058473	4.816018
286.732382	7999.872533	13.429991	-0.058465	4.816007
286.647241	7999.938300	13.434995	-0.058449	4.816027
286.542781	7999.797502	13.440000	-0.058430	4.815986
286.708376	7999.947956	13.445005	-0.058461	4.816029
286.636917	7999.892166	13.450010	-0.058447	4.816013
286.685285	7999.800087	13.455015	-0.058456	4.815986
286.682154	7999.945340	13.460019	-0.058456	4.816029
286.648250	7999.826124	13.465024	-0.058449	4.815994
286.690327	7999.929460	13.470029	-0.058457	4.816024
286.715043	7999.888237	13.475034	-0.058462	4.816012
286.651818	7999.905252	13.480039	-0.058450	4.816017
286.782200	7999.943947	13.485043	-0.058474	4.816028
286.805988	7999.890955	13.490048	-0.058479	4.816012
286.848806	7999.887457	13.495053	-0.058487	4.816011
286.641139	7999.832399	13.500058	-0.058448	4.815996
286.424704	7999.902192	13.505063	-0.058408	4.816017
286.845129	7999.933332	13.510067	-0.058486	4.816024
286.742211	7999.808588	13.515072	-0.058467	4.815988
286.901597	7999.951451	13.520077	-0.058496	4.816029
286.829049	7999.810163	13.525082	-0.058483	4.815988
286.799912	7999.885495	13.530087	-0.058477	4.816010
286.620426	7999.930315	13.535091	-0.058444	4.816025
286.709436	7999.880644	13.540096	-0.058461	4.816010
286.716065	7999.849778	13.545101	-0.058462	4.816000
286.781802	7999.817849	13.550106	-0.058474	4.815991
287.038523	7999.898371	13.555111	-0.058522	4.816013
286.965111	7999.884215	13.560115	-0.058508	4.816009
286.725630	7999.958932	13.565120	-0.058464	4.816032
286.588144	7999.875231	13.570125	-0.058438	4.816009
286.658057	7999.870089	13.575130	-0.058451	4.816007
286.831275	7999.856138	13.580135	-0.058483	4.816002
286.895679	7999.882950	13.585139	-0.058495	4.816009
286.908521	7999.858607	13.590144	-0.058498	4.816002
286.904511	8000.008120	13.595149	-0.058497	4.816046
286.702177	7999.889049	13.600154	-0.058459	4.816012
286.695146	7999.861141	13.605159	-0.058458	4.816004
286.767615	7999.859250	13.610163	-0.058471	4.816003
286.656364	7999.944843	13.615168	-0.058451	4.816029
286.632455	7999.836493	13.620173	-0.058446	4.815997
286.714576	7999.936283	13.625178	-0.058461	4.816026
286.851552	7999.880003	13.630183	-0.058487	4.816009
286.834436	7999.881828	13.635187	-0.058484	4.816009
286.910853	7999.814833	13.640192	-0.058498	4.815989
287.079004	7999.931144	13.645197	-0.058529	4.816022
286.908686	7999.893859	13.650202	-0.058498	4.816012
286.823612	7999.895518	13.655207	-0.058482	4.816013
286.949942	7999.909565	13.660211	-0.058505	4.816017
286.895514	7999.853015	13.665216	-0.058495	4.816000
286.798023	7999.839491	13.670221	-0.058477	4.815997
286.854789	7999.982627	13.675226	-0.058487	4.816039
286.831726	7999.872155	13.680231	-0.058483	4.816006
286.872059	7999.852585	13.685235	-0.058491	4.816000
286.658263	7999.917084	13.690240	-0.058451	4.816020
286.974626	7999.851241	13.695245	-0.058510	4.816000
286.752768	7999.838663	13.700250	-0.058468	4.815997
286.807158	7999.949702	13.705255	-0.058479	4.816029
286.706172	7999.879486	13.710259	-0.058460	4.816009
286.769532	7999.867814	13.715264	-0.058471	4.816005
286.837847	7999.929956	13.720269	-0.058484	4.816023
286.760063	7999.899694	13.725274	-0.058470	4.816015
286.921204	7999.893003	13.730279	-0.058500	4.816012
286.952174	7999.891428	13.735283	-0.058505	4.816011
286.627722	7999.886603	13.740288	-0.058445	4.816012
286.811333	7999.912374	13.745293	-0.058479	4.816018
286.767036	7999.858146	13.750298	-0.058471	4.816003
286.559942	7999.916355	13.755303	-0.058432	4.816021
286.722542	7999.859473	13.760307	-0.058463	4.816003
286.837031	7999.933138	13.765312	-0.058484	4.816024
286.891776	7999.897804	13.770317	-0.058494	4.816014
286.768286	7999.857095	13.775322	-0.058471	4.816002
287.146474	7999.949441	13.780327	-0.058542	4.816027
286.972126	7999.881096	13.785331	-0.058509	4.816008
286.794529	7999.872528	13.790336	-0.058476	4.816007
287.039331	7999.907958	13.795341	-0.058522	4.816016
286.807859	7999.962520	13.800346	-0.058479	4.816033
286.705828	7999.838860	13.805351	-0.058459	4.815997
286.846180	7999.895900	13.810355	-0.058486	4.816013
287.028264	7999.923781	13.815360	-0.058519	4.816020
286.909950	7999.908809	13.820365	-0.058497	4.816017
286.693997	7999.878175	13.825370	-0.058457	4.816009
286.763532	7999.861273	13.830375	-0.058470	4.816004
286.822930	7999.911500	13.835379	-0.058481	4.816018
286.841853	7999.908637	13.840384	-0.058485	4.816017
286.685123	7999.843819	13.845389	-0.058455	4.815999
286.680601	7999.937761	13.850394	-0.058455	4.816026
286.776463	7999.854024	13.855399	-0.058472	4.816001
287.015771	7999.864779	13.860403	-0.058517	4.816003
286.776642	7999.921339	13.865408	-0.058473	4.816021
286.758549	7999.872928	13.870413	-0.058469	4.816007
286.859446	7999.922841	13.875418	-0.058488	4.816021
287.007436	7999.848597	13.880423	-0.058515	4.815999
286.902707	7999.896913	13.885427	-0.058496	4.816013
286.961853	7999.869137	13.890432	-0.058507	4.816005
287.047698	7999.930530	13.895437	-0.058523	4.816022
286.974274	7999.994373	13.900442	-0.058509	4.816041
287.053921	7999.850505	13.905447	-0.058524	4.815999
286.793793	7999.933395	13.910451	-0.058476	4.816025
286.899487	7999.847699	13.915456	-0.058495	4.815999
287.029690	7999.907760	13.920461	-0.058520	4.816016
286.806302	7999.958195	13.925466	-0.058478	4.816032
286.840957	7999.839154	13.930471	-0.058484	4.815997
286.847650	7999.879877	13.935475	-0.058486	4.816009
286.685693	7999.901510	13.940480	-0.058455	4.816016
286.940364	7999.901860	13.945485	-0.058503	4.816015
286.903308	7999.919350	13.950490	-0.058496	4.816020
286.947571	7999.862455	13.955495	-0.058504	4.816003
286.888050	7999.936166	13.960499	-0.058493	4.816025
286.850766	7999.869243	13.965504	-0.058486	4.816005
287.018041	8000.003703	13.970509	-0.058517	4.816044
286.892250	7999.842214	13.975514	-0.058494	4.815997
286.810563	7999.916591	13.980519	-0.058479	4.816020
286.846514	7999.861683	13.985523	-0.058485	4.816003
286.696525	7999.832247	13.990528	-0.058457	4.815995
287.059881	7999.850597	13.995533	-0.058525	4.815999
287.033739	7999.953764	14.000538	-0.058520	4.816029
286.969450	7999.862843	14.005543	-0.058508	4.816003
286.870155	7999.908052	14.010547	-0.058490	4.816017
286.934099	7999.909212	14.015552	-0.058502	4.816017
286.951989	7999.894578	14.020557	-0.058505	4.816012
286.683363	7999.920684	14.025562	-0.058455	4.816021
286.881718	7999.835602	14.030567	-0.058492	4.815995
286.933114	7999.911328	14.035571	-0.058501	4.816017
286.718071	7999.950160	14.040576	-0.058461	4.816030
287.004885	7999.936136	14.045581	-0.058515	4.816024
286.918153	7999.917464	14.050586	-0.058499	4.816019
286.812249	7999.845021	14.055591	-0.058479	4.815999
286.880111	7999.879375	14.060595	-0.058491	4.816008
286.746405	7999.898315	14.065600	-0.058467	4.816015
287.060381	7999.848456	14.070605	-0.058525	4.815998
286.936525	7999.994724	14.075610	-0.058502	4.816042
286.964834	7999.832829	14.080615	-0.058507	4.815994
286.911256	7999.960071	14.085619	-0.058497	4.816032
286.827364	7999.848494	14.090624	-0.058482	4.816000
286.995942	7999.880404	14.095629	-0.058513	4.816008
287.049834	7999.983955	14.100634	-0.058523	4.816038
286.838016	7999.842274	14.105639	-0.058483	4.815998
286.853205	7999.895973	14.110643	-0.058486	4.816013
286.869351	7999.915497	14.115648	-0.058489	4.816019
286.872552	7999.846104	14.120653	-0.058490	4.815999
286.831051	7999.868856	14.125658	-0.058482	4.816005
286.923052	7999.915402	14.130663	-0.058499	4.816019
286.959294	7999.874388	14.135667	-0.058506	4.816006
286.920735	7999.954891	14.140672	-0.058499	4.816030
286.975753	7999.893918	14.145677	-0.058509	4.816012
286.891128	7999.872079	14.150682	-0.058493	4.816006
287.077987	7999.867992	14.155687	-0.058528	4.816004
287.020902	7999.881913	14.160691	-0.058517	4.816008
287.068821	7999.970398	14.165696	-0.058526	4.816034
286.932450	7999.889922	14.170701	-0.058501	4.816011
286.691473	7999.905845	14.175706	-0.058456	4.816017
286.739949	7999.842617	14.180711	-0.058465	4.815998
286.811296	7999.891992	14.185715	-0.058478	4.816012
286.953897	7999.972580	14.190720	-0.058505	4.816035
286.976218	7999.904602	14.195725	-0.058509	4.816015
287.134564	7999.895724	14.200730	-0.058539	4.816012
287.112897	7999.850453	14.205735	-0.058534	4.815999
286.919432	7999.876856	14.210739	-0.058498	4.816007
286.888413	7999.928647	14.215744	-0.058493	4.816023
286.905256	7999.958869	14.220749	-0.058496	4.816031
286.955555	7999.861482	14.225754	-0.058505	4.816003
286.845242	7999.850930	14.230759	-0.058485	4.816000
286.961688	7999.986604	14.235763	-0.058506	4.816039
286.600104	7999.797328	14.240768	-0.058439	4.815986
286.779213	7999.941617	14.245773	-0.058472	4.816027
286.987134	7999.840682	14.250778	-0.058511	4.815996
287.113055	7999.851515	14.255783	-0.058534	4.815999
287.083268	7999.993081	14.260787	-0.058529	4.816040
286.963969	7999.825300	14.265792	-0.058507	4.815992
287.192278	7999.640326	14.270797	-0.058549	4.815937

287.015401	7996.364751	14.275802	-0.058514	4.814981
286.877379	7990.790181	14.280807	-0.058485	4.813352
286.975446	7983.983466	14.285811	-0.058498	4.811361
286.849735	7976.665588	14.290816	-0.058470	4.809221
286.848722	7969.102569	14.295821	-0.058465	4.807007
286.878477	7961.214189	14.300826	-0.058465	4.804697
286.821845	7953.373942	14.305831	-0.058450	4.802401
286.692435	7945.398876	14.310835	-0.058421	4.800064
286.626089	7937.422414	14.315840	-0.058403	4.797725
286.743032	7929.459272	14.320845	-0.058420	4.795388
286.453779	7921.441273	14.325850	-0.058360	4.793036
286.421392	7913.343238	14.330855	-0.058349	4.790658
286.511907	7905.423285	14.335859	-0.058361	4.788331
286.395476	7897.355267	14.340864	-0.058334	4.785960
286.376584	7889.428650	14.345869	-0.058325	4.783628
286.324454	7881.409939	14.350874	-0.058310	4.781269
286.678869	7873.428909	14.355879	-0.058371	4.778918
286.478058	7865.479447	14.360883	-0.058328	4.776577
286.080301	7857.398682	14.365888	-0.058249	4.774198
286.358160	7849.389059	14.370893	-0.058296	4.771835
286.274769	7841.446920	14.375898	-0.058275	4.769493
286.007238	7833.420464	14.380903	-0.058220	4.767125
286.009371	7825.384943	14.385907	-0.058215	4.764752
285.924871	7817.430428	14.390912	-0.058194	4.762403
285.794438	7809.395836	14.395917	-0.058165	4.760028
285.725698	7801.407295	14.400922	-0.058146	4.757666
285.658036	7793.342597	14.405927	-0.058129	4.755280
285.598458	7785.408613	14.410931	-0.058112	4.752932
285.536259	7777.302551	14.415936	-0.058095	4.750531
285.697318	7769.362472	14.420941	-0.058120	4.748178
285.696999	7761.331637	14.425946	-0.058115	4.745797
285.487210	7753.342285	14.430951	-0.058071	4.743428
285.595688	7745.372385	14.435955	-0.058086	4.741063
285.407831	7737.314644	14.440960	-0.058045	4.738671
285.338581	7729.351733	14.445965	-0.058027	4.736306
285.328282	7721.350446	14.450970	-0.058020	4.733928
285.302485	7713.338325	14.455975	-0.058010	4.731545
285.209546	7705.302245	14.460979	-0.057988	4.729155
284.972795	7697.306474	14.465984	-0.057938	4.726776
285.266818	7689.312055	14.470989	-0.057988	4.724394
285.134902	7681.371614	14.475994	-0.057958	4.722028
284.956349	7673.297582	14.480999	-0.057920	4.719622
284.917859	7665.371461	14.486003	-0.057907	4.717258
284.918225	7657.309563	14.491008	-0.057902	4.714852
285.015522	7649.308125	14.496013	-0.057915	4.712463
284.812356	7641.327743	14.501018	-0.057872	4.710079
284.668092	7633.292504	14.506023	-0.057840	4.707678
284.593608	7625.305896	14.511027	-0.057821	4.705290
284.306602	7617.319421	14.516032	-0.057762	4.702902
284.588607	7609.337856	14.521037	-0.057809	4.700512
284.666873	7601.339775	14.526042	-0.057819	4.698116
284.706660	7593.279810	14.531047	-0.057821	4.695701
284.645109	7585.348106	14.536051	-0.057804	4.693323
284.673750	7577.231774	14.541056	-0.057804	4.690889
284.661912	7569.317993	14.546061	-0.057797	4.688514
284.487548	7561.282281	14.551066	-0.057759	4.686101
284.417417	7553.279593	14.556071	-0.057741	4.683697
284.346782	7545.368274	14.561075	-0.057723	4.681320
284.218674	7537.320498	14.566080	-0.057693	4.678900
284.306905	7529.327142	14.571085	-0.057705	4.676495
284.262611	7521.255106	14.576090	-0.057691	4.674065
284.063906	7513.160418	14.581095	-0.057649	4.671627
284.081750	7505.224647	14.586099	-0.057647	4.669236
284.207582	7497.169353	14.591104	-0.057665	4.666807
284.203614	7489.223012	14.596109	-0.057659	4.664410
284.122485	7481.271034	14.601114	-0.057639	4.662010
283.978996	7473.186425	14.606119	-0.057607	4.659569
284.089973	7465.273738	14.611123	-0.057622	4.657178
283.939419	7457.284292	14.616128	-0.057589	4.654763
284.000352	7449.268063	14.621133	-0.057595	4.652339
284.051329	7441.207475	14.626138	-0.057600	4.649899
284.040561	7433.272486	14.631143	-0.057592	4.647497
283.850233	7425.276989	14.636147	-0.057552	4.645075
283.632939	7417.283578	14.641152	-0.057506	4.642653
283.721422	7409.195733	14.646157	-0.057517	4.640200
283.595434	7401.253347	14.651162	-0.057489	4.637791
283.472155	7393.203080	14.656167	-0.057460	4.635347
283.497952	7385.225409	14.661171	-0.057460	4.632924
283.310576	7377.165004	14.666176	-0.057420	4.630475
283.362305	7369.188650	14.671181	-0.057424	4.628050
283.281299	7361.179188	14.676186	-0.057404	4.625613
283.167977	7353.210827	14.681191	-0.057378	4.623188
283.244160	7345.216363	14.686195	-0.057387	4.620754
283.132551	7337.170403	14.691200	-0.057361	4.618302
283.226736	7329.204898	14.696205	-0.057373	4.615874
282.994845	7321.205177	14.701210	-0.057324	4.613434
282.966669	7313.146659	14.706215	-0.057314	4.610975
282.956355	7305.179370	14.711219	-0.057307	4.608542
282.798339	7297.143614	14.716224	-0.057272	4.606087
282.905452	7289.129783	14.721229	-0.057287	4.603638
282.909478	7281.182378	14.726234	-0.057282	4.601207
282.843212	7273.183047	14.731239	-0.057265	4.598760
282.865862	7265.228809	14.736243	-0.057264	4.596324
282.603150	7257.172809	14.741248	-0.057210	4.593857
282.782630	7249.156815	14.746253	-0.057238	4.591400
282.749121	7241.140040	14.751258	-0.057226	4.588942
282.692172	7233.135734	14.756263	-0.057211	4.586486
282.798272	7225.179343	14.761267	-0.057225	4.584044
282.644070	7217.154239	14.766272	-0.057191	4.581579
282.511369	7209.176157	14.771277	-0.057161	4.579127
282.724147	7201.182656	14.776282	-0.057196	4.576670
282.805715	7193.146905	14.781287	-0.057206	4.574198
282.754549	7185.174519	14.786291	-0.057191	4.571744
282.494173	7177.124754	14.791296	-0.057137	4.569265
282.236047	7169.165563	14.796301	-0.057084	4.566812
282.422572	7161.105448	14.801306	-0.057113	4.564327
282.278521	7153.114236	14.806311	-0.057081	4.561862
282.427368	7145.137738	14.811315	-0.057104	4.559400
282.274935	7137.168396	14.816320	-0.057070	4.556939
282.165486	7129.126520	14.821325	-0.057045	4.554454
282.215537	7121.105721	14.826330	-0.057049	4.551975
282.000970	7113.089198	14.831335	-0.057004	4.549495
282.049840	7105.143737	14.836339	-0.057007	4.547036
282.065506	7097.081735	14.841344	-0.057005	4.544540
281.966021	7089.164666	14.846349	-0.056981	4.542087
281.903304	7081.116844	14.851354	-0.056965	4.539592
281.908258	7073.158713	14.856359	-0.056960	4.537124
281.814024	7065.141013	14.861363	-0.056937	4.534636
281.826562	7057.097084	14.866368	-0.056935	4.532138
281.864981	7049.113722	14.871373	-0.056936	4.529658
281.776968	7041.137398	14.876378	-0.056915	4.527178
281.701721	7033.084130	14.881383	-0.056896	4.524674
281.397192	7025.164034	14.886387	-0.056834	4.522208
281.551422	7017.094337	14.891392	-0.056857	4.519696
281.517357	7009.146430	14.896397	-0.056846	4.517220
281.347044	7001.083591	14.901402	-0.056809	4.514707
281.205843	6992.989105	14.906407	-0.056777	4.512182
281.298120	6985.044696	14.911411	-0.056789	4.509703
281.272364	6977.043454	14.916416	-0.056779	4.507205
281.369428	6969.048802	14.921421	-0.056792	4.504707
281.197327	6961.137381	14.926426	-0.056755	4.502234
281.249738	6953.071040	14.931431	-0.056759	4.499712
281.305133	6945.147830	14.936435	-0.056764	4.497232
281.157188	6937.064082	14.941440	-0.056732	4.494701
281.288603	6929.075379	14.946445	-0.056751	4.492199
281.202895	6921.136675	14.951450	-0.056730	4.489710
280.844091	6913.072341	14.956455	-0.056658	4.487180
280.890611	6905.012215	14.961459	-0.056661	4.484651
280.636970	6897.081529	14.966464	-0.056609	4.482160
280.669106	6889.044503	14.971469	-0.056609	4.479636
280.630481	6881.082160	14.976474	-0.056597	4.477133
280.612190	6873.058604	14.981479	-0.056588	4.474609
280.584751	6865.051580	14.986483	-0.056578	4.472089
280.400068	6856.962399	14.991488	-0.056538	4.469542
280.610610	6849.031501	14.996493	-0.056572	4.467044
280.468620	6841.020417	15.001498	-0.056541	4.464518
280.487889	6833.066691	15.006503	-0.056539	4.462010
280.383758	6825.039616	15.011507	-0.056514	4.459476
280.272050	6817.051830	15.016512	-0.056488	4.456954
280.304559	6809.035431	15.021517	-0.056489	4.454421
280.327036	6801.033571	15.026522	-0.056488	4.451892
280.012358	6793.011457	15.031527	-0.056424	4.449353
279.992741	6785.067581	15.036531	-0.056415	4.446839
279.966989	6777.005082	15.041536	-0.056405	4.444286
280.006283	6769.041027	15.046541	-0.056408	4.441763
279.897614	6761.045868	15.051546	-0.056382	4.439227
279.718904	6753.016831	15.056551	-0.056344	4.436680
279.834325	6745.009463	15.061555	-0.056360	4.434139
279.929828	6736.929259	15.066560	-0.056372	4.431573
279.679368	6728.973081	15.071565	-0.056321	4.429044
279.720659	6720.977493	15.076570	-0.056323	4.426502
279.776508	6712.984334	15.081575	-0.056328	4.423960
279.757633	6704.978132	15.086579	-0.056319	4.421411
279.480010	6697.005575	15.091584	-0.056263	4.418871
279.687219	6688.993788	15.096589	-0.056296	4.416319
279.795834	6681.007520	15.101594	-0.056311	4.413773
279.494512	6672.949489	15.106599	-0.056250	4.411200
279.461685	6665.014622	15.111603	-0.056238	4.408667
279.515112	6656.942368	15.116608	-0.056243	4.406089
279.630642	6648.949099	15.121613	-0.056259	4.403535
279.366917	6640.987600	15.126618	-0.056205	4.400988
279.224184	6633.001671	15.131623	-0.056173	4.398432
279.139254	6625.035155	15.136627	-0.056152	4.395881
279.004653	6616.963987	15.141632	-0.056122	4.393294
279.067984	6608.958770	15.146637	-0.056128	4.390729
279.156381	6600.970465	15.151642	-0.056140	4.388167
279.041928	6592.943400	15.156647	-0.056113	4.385591
279.147213	6585.047751	15.161651	-0.056127	4.383056
278.890076	6576.978076	15.166656	-0.056074	4.380462
278.689800	6569.032723	15.171661	-0.056032	4.377906
278.629491	6561.000456	15.176666	-0.056015	4.375322
278.642387	6553.003709	15.181671	-0.056013	4.372749
278.774821	6544.956295	15.186675	-0.056032	4.370158
278.625380	6536.985390	15.191680	-0.055999	4.367588
278.759349	6528.948387	15.196685	-0.056019	4.364998
278.722013	6521.051721	15.201690	-0.056006	4.362450
278.442561	6512.958150	15.206695	-0.055949	4.359835
278.551694	6505.055674	15.211699	-0.055964	4.357283
278.402773	6496.988755	15.216704	-0.055931	4.354675
278.441140	6488.877868	15.221709	-0.055933	4.352052
278.404140	6480.892890	15.226714	-0.055921	4.349468
278.181112	6472.913347	15.231719	-0.055874	4.346883
278.158717	6464.947295	15.236723	-0.055865	4.344302
278.199050	6456.955886	15.241728	-0.055867	4.341712
278.134525	6448.930892	15.246733	-0.055850	4.339109
278.286657	6440.981443	15.251738	-0.055873	4.336530
278.136822	6432.936063	15.256743	-0.055840	4.333916
278.006271	6424.912502	15.261747	-0.055810	4.331308
278.011966	6416.944796	15.266752	-0.055806	4.328717
278.035403	6408.960394	15.271757	-0.055805	4.326120
278.077185	6400.966981	15.276762	-0.055808	4.323518
278.002858	6392.957822	15.281767	-0.055789	4.320908
278.091050	6384.997961	15.286771	-0.055800	4.318315
277.915613	6376.939417	15.291776	-0.055762	4.315685
277.821090	6368.952015	15.296781	-0.055739	4.313078
277.806212	6360.874076	15.301786	-0.055731	4.310440
277.669869	6352.918405	15.306791	-0.055701	4.307840
277.725702	6344.929911	15.311795	-0.055706	4.305229
277.621441	6336.940302	15.316800	-0.055681	4.302614
277.575194	6328.924727	15.321805	-0.055668	4.299990
277.405506	6320.990265	15.326810	-0.055631	4.297390
277.396050	6312.935092	15.331815	-0.055624	4.294750
277.471068	6304.921943	15.336819	-0.055632	4.292123
277.307728	6296.880264	15.341824	-0.055597	4.289483
277.117728	6288.947852	15.346829	-0.055556	4.286877
277.277510	6280.931268	15.351834	-0.055581	4.284245
277.078120	6272.934825	15.356839	-0.055538	4.281614
277.061585	6264.948447	15.361843	-0.055530	4.278987
276.931264	6256.896750	15.366848	-0.055501	4.276336
277.119584	6248.907657	15.371853	-0.055530	4.273706
277.057578	6240.873743	15.376858	-0.055514	4.271058
276.966438	6232.870181	15.381863	-0.055491	4.268418
276.986731	6224.893402	15.386867	-0.055490	4.265787
276.707600	6216.895114	15.391872	-0.055433	4.263143
276.795240	6208.920869	15.396877	-0.055444	4.260510
276.986648	6200.902591	15.401882	-0.055474	4.257861
276.673758	6192.908932	15.406887	-0.055411	4.255214
276.743147	6184.901894	15.411891	-0.055419	4.252564
276.530112	6176.881827	15.416896	-0.055374	4.249906
276.563398	6168.898003	15.421901	-0.055375	4.247261
276.430134	6160.916072	15.426906	-0.055345	4.244612
276.417304	6152.956633	15.431911	-0.055337	4.241971
276.575630	6144.974019	15.436915	-0.055361	4.239322
276.424207	6136.933410	15.441920	-0.055328	4.236649
276.291568	6128.915265	15.446925	-0.055298	4.233983
276.278724	6120.884840	15.451930	-0.055290	4.231311
276.293039	6112.901872	15.456935	-0.055288	4.228654
276.405489	6104.897738	15.461939	-0.055303	4.225989
276.198443	6096.955418	15.466944	-0.055260	4.223340
276.174187	6088.929674	15.471949	-0.055250	4.220663
275.970904	6080.974967	15.476954	-0.055207	4.218007
275.923588	6072.890940	15.481959	-0.055193	4.215307
275.954461	6064.930337	15.486963	-0.055193	4.212647
275.824343	6056.902928	15.491968	-0.055164	4.209962
275.883124	6048.955358	15.496973	-0.055170	4.207304
275.975587	6040.935350	15.501978	-0.055182	4.204620
275.681115	6032.933854	15.506983	-0.055122	4.201936
275.770634	6024.946536	15.511987	-0.055133	4.199260
275.795809	6016.959716	15.516992	-0.055133	4.196581
275.792117	6008.889603	15.521997	-0.055127	4.193872
275.888347	6000.833731	15.527002	-0.055139	4.191168
275.720522	5992.831107	15.532007	-0.055103	4.188477
275.559837	5984.921648	15.537011	-0.055068	4.185815
275.620295	5976.913926	15.542016	-0.055074	4.183121
275.670611	5968.877370	15.547021	-0.055078	4.180416
275.481328	5960.957325	15.552026	-0.055037	4.177745
275.359584	5952.865327	15.557031	-0.055009	4.175016
275.387993	5944.920032	15.562035	-0.055010	4.172335
275.254471	5936.869495	15.567040	-0.054979	4.169616
275.214732	5928.896068	15.572045	-0.054967	4.166922
275.223807	5920.905917	15.577050	-0.054963	4.164221
274.921592	5912.945926	15.582055	-0.054902	4.161525
275.185966	5904.919051	15.587059	-0.054946	4.158811
275.185271	5896.928228	15.592064	-0.054940	4.156105
274.925157	5888.885897	15.597069	-0.054887	4.153376
274.891117	5880.863460	15.602074	-0.054875	4.150655
274.888500	5872.882951	15.607079	-0.054870	4.147947
274.812461	5864.868800	15.612083	-0.054850	4.145224
274.820108	5856.867196	15.617088	-0.054846	4.142505
274.746999	5848.891982	15.622093	-0.054828	4.139793
274.960110	5840.923149	15.627098	-0.054862	4.137084
274.699297	5832.855847	15.632103	-0.054808	4.134334
274.730694	5824.865341	15.637107	-0.054809	4.131612
274.785638	5816.853636	15.642112	-0.054814	4.128881
274.647382	5808.883318	15.647117	-0.054783	4.126160
274.436192	5800.920000	15.652122	-0.054738	4.123439
274.360836	5792.890487	15.657127	-0.054719	4.120695
274.533494	5784.914970	15.662131	-0.054746	4.117971
274.359562	5776.890582	15.667136	-0.054708	4.115224
274.498522	5768.834740	15.672141	-0.054729	4.112468
274.608838	5760.826296	15.677146	-0.054744	4.109726
274.317422	5752.842456	15.682151	-0.054685	4.106986
274.457465	5744.866350	15.687155	-0.054706	4.104252
274.413058	5736.894167	15.692160	-0.054692	4.101515
274.031521	5728.917184	15.697165	-0.054616	4.098771
274.044333	5720.937285	15.702170	-0.054613	4.096029
273.841466	5712.893722	15.707175	-0.054570	4.093260
274.000609	5704.917253	15.712179	-0.054595	4.090517
273.773781	5696.908207	15.717184	-0.054547	4.087756
273.686973	5688.902034	15.722189	-0.054526	4.084995
273.806074	5680.951317	15.727194	-0.054543	4.082255
273.590776	5672.903962	15.732199	-0.054497	4.079475
273.541874	5664.958758	15.737203	-0.054483	4.076731
273.574167	5656.899250	15.742208	-0.054484	4.073947
273.549303	5648.867346	15.747213	-0.054474	4.071169
273.421645	5640.908132	15.752218	-0.054445	4.068413
273.427726	5632.882372	15.757223	-0.054441	4.065634
273.661804	5624.963812	15.762227	-0.054479	4.062894
273.498378	5616.901694	15.767232	-0.054444	4.060096
273.432765	5608.985192	15.772237	-0.054426	4.057348
273.431043	5600.951056	15.777242	-0.054421	4.054559
273.093745	5592.917223	15.782247	-0.054353	4.051763
273.109308	5584.929440	15.787251	-0.054350	4.048986
273.164110	5576.928486	15.792256	-0.054355	4.046203
273.224080	5568.903227	15.797261	-0.054361	4.043410
273.122323	5560.931396	15.802266	-0.054337	4.040631
272.970063	5552.927812	15.807271	-0.054303	4.037838
273.033561	5544.942291	15.812275	-0.054310	4.035053
272.916582	5536.821451	15.817280	-0.054283	4.032216
273.039166	5528.825805	15.822285	-0.054301	4.029424
273.045335	5520.879866	15.827290	-0.054297	4.026646
272.698177	5512.878630	15.832295	-0.054227	4.023842
272.861241	5504.927274	15.837299	-0.054252	4.021061
272.758497	5496.908150	15.842304	-0.054227	4.018249
272.686558	5488.897810	15.847309	-0.054209	4.015440
272.598547	5480.928503	15.852314	-0.054187	4.012643
272.452761	5472.864198	15.857319	-0.054155	4.009809
272.593401	5464.912166	15.862323	-0.054176	4.007017
272.525800	5456.882454	15.867328	-0.054158	4.004193
272.487162	5448.938773	15.872333	-0.054146	4.001398
272.536339	5440.935612	15.877338	-0.054150	3.998581
272.526049	5432.916807	15.882343	-0.054142	3.995755
272.373388	5424.900315	15.887347	-0.054109	3.992927
272.301507	5416.888602	15.892352	-0.054090	3.990099
272.371775	5408.870008	15.897357	-0.054098	3.987269
272.404087	5400.880003	15.902362	-0.054099	3.984446
272.038663	5392.940225	15.907367	-0.054026	3.981633
272.295848	5384.953962	15.912371	-0.054068	3.978811
272.112476	5376.939711	15.917376	-0.054029	3.975970
272.065128	5368.932050	15.922381	-0.054015	3.973132
271.993561	5360.927739	15.927386	-0.053996	3.970293
271.784902	5352.952273	15.932391	-0.053952	3.967459
271.847272	5344.952375	15.937395	-0.053959	3.964619
271.764863	5336.969366	15.942400	-0.053938	3.961781
271.769053	5328.959961	15.947405	-0.053934	3.958933
271.797551	5321.004287	15.952410	-0.053934	3.956102
271.735792	5312.914865	15.957415	-0.053917	3.953220
271.867128	5304.911498	15.962419	-0.053936	3.950370
271.666521	5296.903485	15.967424	-0.053894	3.947511
271.608078	5288.929515	15.972429	-0.053877	3.944664
271.572847	5281.000409	15.977434	-0.053866	3.941831
271.474804	5272.948218	15.982439	-0.053842	3.938952
271.372225	5264.986820	15.987443	-0.053818	3.936102
271.198082	5257.007702	15.992448	-0.053780	3.933243
271.310788	5248.960294	15.997453	-0.053796	3.930362
271.407632	5240.976115	16.002458	-0.053809	3.927502
271.148023	5232.909190	16.007463	-0.053755	3.924603
271.210852	5225.002739	16.012467	-0.053762	3.921766
271.112557	5216.984920	16.017472	-0.053738	3.918884
271.150014	5208.984493	16.022477	-0.053740	3.916008
271.116944	5200.999544	16.027482	-0.053729	3.913135
271.130577	5192.919317	16.032487	-0.053726	3.910226
271.100316	5184.985039	16.037491	-0.053715	3.907366
271.019167	5176.963967	16.042496	-0.053695	3.904472
270.956719	5168.996362	16.047501	-0.053678	3.901596
270.809665	5160.994919	16.052506	-0.053645	3.898704
270.854453	5152.973226	16.057511	-0.053648	3.895806
270.959557	5144.979405	16.062515	-0.053663	3.892917
270.759026	5136.934863	16.067520	-0.053620	3.890001
270.650089	5128.978711	16.072525	-0.053595	3.887118
270.587556	5120.983050	16.077530	-0.053578	3.884218
270.497865	5112.969863	16.082535	-0.053556	3.881310
270.631464	5105.008602	16.087539	-0.053576	3.878422
270.309637	5097.000769	16.092544	-0.053510	3.875507
270.510216	5088.802366	16.097549	-0.053542	3.872530
270.565247	5080.810906	16.102554	-0.053547	3.869623
270.273772	5072.896185	16.107559	-0.053488	3.866736
270.508007	5064.925127	16.112563	-0.053526	3.863836
270.407250	5056.952271	16.117568	-0.053502	3.860926
270.276878	5048.967402	16.122573	-0.053473	3.858010
270.256954	5040.968989	16.127578	-0.053464	3.855088
270.263422	5032.959853	16.132583	-0.053460	3.852161
270.046871	5024.963837	16.137587	-0.053414	3.849232
269.799970	5016.963732	16.142592	-0.053363	3.846299
269.902504	5008.985601	16.147597	-0.053377	3.843378
269.822010	5001.016763	16.152602	-0.053357	3.840455
269.631709	4993.020974	16.157607	-0.053316	3.837517
269.721349	4985.014174	16.162611	-0.053328	3.834579
269.904431	4976.987049	16.167616	-0.053357	3.831633
269.768762	4968.988913	16.172621	-0.053326	3.828689
269.748309	4961.014283	16.177626	-0.053317	3.825754
269.714174	4952.988940	16.182631	-0.053305	3.822797
269.655897	4945.049929	16.187635	-0.053289	3.819870
269.509436	4937.066191	16.192640	-0.053257	3.816922
269.421661	4929.066760	16.197645	-0.053235	3.813967
269.538035	4921.049266	16.202650	-0.053252	3.811007
269.388811	4913.046396	16.207655	-0.053219	3.808045
269.409570	4905.071273	16.212659	-0.053217	3.805094
269.371261	4897.108264	16.217664	-0.053205	3.802145
269.047228	4889.087129	16.222669	-0.053140	3.799165
268.993029	4881.113164	16.227674	-0.053124	3.796206
268.868647	4873.056207	16.232679	-0.053096	3.793213
268.988252	4865.051074	16.237683	-0.053113	3.790242
268.904726	4857.027974	16.242688	-0.053092	3.787257
268.938869	4849.031167	16.247693	-0.053093	3.784282
268.972014	4841.080090	16.252698	-0.053094	3.781323
268.767873	4833.078922	16.257703	-0.053051	3.778336
268.741938	4825.068578	16.262707	-0.053041	3.775348
268.779965	4817.092557	16.267712	-0.053043	3.772372
268.586993	4809.058925	16.272717	-0.053002	3.769367
268.693445	4801.106504	16.277722	-0.053016	3.766396
268.560630	4793.071275	16.282727	-0.052986	3.763387
268.467953	4785.102624	16.287731	-0.052964	3.760401
268.330871	4777.133876	16.292736	-0.052933	3.757412
268.251249	4769.095654	16.297741	-0.052913	3.754395
268.576073	4761.073388	16.302746	-0.052968	3.751392
268.452485	4753.051580	16.307751	-0.052940	3.748375
268.439185	4745.076845	16.312755	-0.052932	3.745377
268.408459	4737.110409	16.317760	-0.052921	3.742379
268.403775	4729.091586	16.322765	-0.052915	3.739359
268.225386	4721.157902	16.327770	-0.052877	3.736365
268.003946	4713.121631	16.332775	-0.052830	3.733329
268.293551	4705.071751	16.337779	-0.052879	3.730297
268.046026	4697.130413	16.342784	-0.052828	3.727292
267.976326	4689.124199	16.347789	-0.052810	3.724263
268.020980	4681.185799	16.352794	-0.052813	3.721260
267.795284	4673.182665	16.357799	-0.052766	3.718224
267.874249	4665.179254	16.362803	-0.052775	3.715193
267.763909	4657.070128	16.367808	-0.052749	3.712114
267.623505	4649.084783	16.372813	-0.052718	3.709079
267.529421	4641.144152	16.377818	-0.052695	3.706060
267.483860	4633.134713	16.382823	-0.052681	3.703013
267.664193	4625.137065	16.387827	-0.052710	3.699974
267.712049	4617.197054	16.392832	-0.052713	3.696951
267.371695	4609.182999	16.397837	-0.052645	3.693887
267.502498	4601.167299	16.402842	-0.052664	3.690833
267.352195	4593.158477	16.407847	-0.052631	3.687771
267.462664	4585.173674	16.412851	-0.052646	3.684722
267.367903	4577.239048	16.417856	-0.052623	3.681685
267.362817	4569.215456	16.422861	-0.052617	3.678614
267.045373	4561.250076	16.427866	-0.052553	3.675554
267.124224	4553.182311	16.432871	-0.052562	3.672463
267.286732	4545.180018	16.437875	-0.052587	3.669396
267.183928	4537.223084	16.442880	-0.052563	3.666337
267.098552	4529.227029	16.447885	-0.052542	3.663261
266.822716	4521.222870	16.452890	-0.052485	3.660175
266.837300	4513.237754	16.457895	-0.052483	3.657101
266.670950	4505.225345	16.462899	-0.052447	3.654009
266.800602	4497.201482	16.467904	-0.052465	3.650917
266.868914	4489.203057	16.472909	-0.052473	3.647832
266.863498	4481.221217	16.477914	-0.052467	3.644748
266.752800	4473.281539	16.482919	-0.052441	3.641675
266.763225	4465.257311	16.487923	-0.052438	3.638570
266.745409	4457.285370	16.492928	-0.052429	3.635481
266.514011	4449.242278	16.497933	-0.052381	3.632357
266.592133	4441.217924	16.502938	-0.052390	3.629246
266.515101	4433.203077	16.507943	-0.052370	3.626131
266.462465	4425.261719	16.512947	-0.052355	3.623043
266.385134	4417.257473	16.517952	-0.052336	3.619927
266.442526	4409.294882	16.522957	-0.052341	3.616829
266.408337	4401.292622	16.527962	-0.052330	3.613710
266.196083	4393.266527	16.532967	-0.052285	3.610574
266.106510	4385.309262	16.537971	-0.052263	3.607465
266.251860	4377.284084	16.542976	-0.052285	3.604334
266.010425	4369.346546	16.547981	-0.052235	3.601223
265.968998	4361.376332	16.552986	-0.052222	3.598103
265.747870	4353.355682	16.557991	-0.052175	3.594955
265.932888	4345.329226	16.562995	-0.052205	3.591813
265.915899	4337.330468	16.568000	-0.052196	3.588674
265.877757	4329.327522	16.573005	-0.052184	3.585530
265.898433	4321.390915	16.578010	-0.052183	3.582411
265.784069	4313.368596	16.583015	-0.052156	3.579251
265.881905	4305.392815	16.588019	-0.052169	3.576113
265.802722	4297.378981	16.593024	-0.052149	3.572953
265.656727	4289.351803	16.598029	-0.052117	3.569782
265.713383	4281.419864	16.603034	-0.052122	3.566652
265.397208	4273.413826	16.608039	-0.052058	3.563479
265.657019	4265.395900	16.613043	-0.052101	3.560315
265.510887	4257.445445	16.618048	-0.052069	3.557163
265.358588	4249.393089	16.623053	-0.052035	3.553968
265.391589	4241.295859	16.628058	-0.052036	3.550758
265.126726	4233.337980	16.633063	-0.051981	3.547591
265.252028	4225.359253	16.638067	-0.052000	3.544425
265.211374	4217.392852	16.643072	-0.051987	3.541256
265.154354	4209.394053	16.648077	-0.051971	3.538070
265.137249	4201.428497	16.653082	-0.051963	3.534897
264.962664	4193.395793	16.658087	-0.051925	3.531688
265.026443	4185.390139	16.663091	-0.051931	3.528495
264.907047	4177.428128	16.668096	-0.051904	3.525311
264.900574	4169.441448	16.673101	-0.051898	3.522118
264.839292	4161.492673	16.678106	-0.051881	3.518935
264.775312	4153.491339	16.683111	-0.051864	3.515728
264.749627	4145.469526	16.688115	-0.051854	3.512511
264.788593	4137.434605	16.693120	-0.051856	3.509288
264.450136	4129.470042	16.698125	-0.051788	3.506078
264.500679	4121.503351	16.703130	-0.051792	3.502877
264.525901	4113.495460	16.708135	-0.051791	3.499655
264.450118	4105.542992	16.713139	-0.051772	3.496450
264.411513	4097.529970	16.718144	-0.051760	3.493218
264.428489	4089.482969	16.723149	-0.051758	3.489972
264.292670	4081.534874	16.728154	-0.051727	3.486757
264.086556	4073.551006	16.733159	-0.051683	3.483523
264.097015	4065.569355	16.738163	-0.051680	3.480294
264.026648	4057.633783	16.743168	-0.051662	3.477078
264.265424	4049.510510	16.748173	-0.051701	3.473792
264.178117	4041.549599	16.753178	-0.051680	3.470559
264.069225	4033.535616	16.758183	-0.051654	3.467301
264.168796	4025.543488	16.763187	-0.051667	3.464055
264.037034	4017.603936	16.768192	-0.051638	3.460820
264.089190	4009.580687	16.773197	-0.051642	3.457553
263.880544	4001.623987	16.778202	-0.051598	3.454303
263.587879	3993.622689	16.783207	-0.051538	3.451028
263.762052	3985.610960	16.788211	-0.051566	3.447761
263.951816	3977.590999	16.793216	-0.051596	3.444488
263.627700	3969.638099	16.798221	-0.051530	3.441223
263.449297	3961.663666	16.803226	-0.051492	3.437951
263.556315	3953.632049	16.808231	-0.051506	3.434661
263.387049	3945.651696	16.813235	-0.051470	3.431380
263.306834	3937.633107	16.818240	-0.051450	3.428083
263.399893	3929.622625	16.823245	-0.051462	3.424792
263.386829	3921.677718	16.828250	-0.051454	3.421522
263.222560	3913.677015	16.833255	-0.051418	3.418220
263.195759	3905.681963	16.838259	-0.051408	3.414922
263.152297	3897.679387	16.843264	-0.051395	3.411617
263.195743	3889.681982	16.848269	-0.051398	3.408314
263.108111	3881.709145	16.853274	-0.051376	3.405013
263.257521	3873.744113	16.858279	-0.051399	3.401721
263.256385	3865.766805	16.863283	-0.051393	3.398415
262.932806	3857.795424	16.868288	-0.051328	3.395097
262.760331	3849.699188	16.873293	-0.051290	3.391729
262.759425	3841.701137	16.878298	-0.051285	3.388405
262.636650	3833.694120	16.883303	-0.051257	3.385069
262.487748	3825.756439	16.888307	-0.051224	3.381759
262.656003	3817.751334	16.893312	-0.051250	3.378427
262.676909	3809.764201	16.898317	-0.051249	3.375095
262.539541	3801.787089	16.903322	-0.051218	3.371759
262.492142	3793.756604	16.908327	-0.051204	3.368399
262.761703	3785.790071	16.913331	-0.051249	3.365075
262.332612	3777.874213	16.918336	-0.051164	3.361743
262.337234	3769.831284	16.923341	-0.051159	3.358370
262.542946	3761.835781	16.928346	-0.051193	3.355021
262.294438	3753.823131	16.933351	-0.051141	3.351646
262.362261	3745.821991	16.938355	-0.051148	3.348283
262.338328	3737.853787	16.943360	-0.051139	3.344927
262.218634	3729.879626	16.948365	-0.051111	3.341562
262.093712	3721.916968	16.953370	-0.051083	3.338198
261.939194	3713.899940	16.958375	-0.051049	3.334806
261.906320	3705.903486	16.963379	-0.051037	3.331424
261.935783	3697.889112	16.968384	-0.051038	3.328034
261.884638	3689.881072	16.973389	-0.051023	3.324640
261.960968	3681.949592	16.978394	-0.051032	3.321279
262.006744	3673.944976	16.983399	-0.051035	3.317883
261.771535	3665.957738	16.988403	-0.050986	3.314480
261.727321	3657.937837	16.993408	-0.050973	3.311067
261.658292	3649.919621	16.998413	-0.050955	3.307651
261.605462	3641.966133	17.003418	-0.050940	3.304259
261.425164	3633.986768	17.008423	-0.050901	3.300847
261.415511	3626.010121	17.013427	-0.050894	3.297440
261.459477	3618.006315	17.018432	-0.050897	3.294019
261.220101	3610.004671	17.023437	-0.050847	3.290586
261.171191	3602.061515	17.028442	-0.050833	3.287180
261.047543	3594.034354	17.033447	-0.050805	3.283733
261.089698	3586.046621	17.038451	-0.050807	3.280305
261.050321	3578.081800	17.043456	-0.050795	3.276880
260.998467	3570.051753	17.048461	-0.050780	3.273423
260.901748	3562.070486	17.053466	-0.050757	3.269982
260.942376	3554.077302	17.058471	-0.050759	3.266537
261.038566	3546.085334	17.063475	-0.050772	3.263091
260.778242	3538.110284	17.068480	-0.050718	3.259635
260.810307	3530.146090	17.073485	-0.050719	3.256191
260.781925	3522.138887	17.078490	-0.050708	3.252723
261.004354	3514.089982	17.083495	-0.050744	3.249243
260.861205	3506.140582	17.088499	-0.050712	3.245788
260.722026	3498.194326	17.093504	-0.050681	3.242331
260.612319	3490.181436	17.098509	-0.050656	3.238842
260.636686	3482.238000	17.103514	-0.050655	3.235385
260.386987	3474.176549	17.108519	-0.050603	3.231862
260.407998	3466.166921	17.113523	-0.050602	3.228368
260.385783	3458.179251	17.118528	-0.050593	3.224879
260.248513	3450.226629	17.123533	-0.050562	3.221396
260.282004	3442.258941	17.128538	-0.050563	3.217910
259.947082	3434.242375	17.133543	-0.050495	3.214384
260.011012	3426.245864	17.138547	-0.050502	3.210879
259.992044	3418.273637	17.143552	-0.050493	3.207377
260.029883	3410.238789	17.148557	-0.050495	3.203846
259.894522	3402.302099	17.153562	-0.050465	3.200348
259.918696	3394.324419	17.158567	-0.050464	3.196834
259.902412	3386.311217	17.163571	-0.050456	3.193299
259.861584	3378.297210	17.168576	-0.050443	3.189759
259.900113	3370.297303	17.173581	-0.050445	3.186224
260.070697	3362.338130	17.178586	-0.050471	3.182709
259.946959	3354.351604	17.183591	-0.050443	3.179165
259.758186	3346.390804	17.188595	-0.050403	3.175626
259.798443	3338.398806	17.193600	-0.050405	3.172080
259.568533	3330.386863	17.198605	-0.050357	3.168508
259.827765	3322.384790	17.203610	-0.050400	3.164958
259.552558	3314.455588	17.208615	-0.050344	3.161414
259.358308	3306.480043	17.213619	-0.050302	3.157848
259.457759	3298.484540	17.218624	-0.050316	3.154282
259.332023	3290.417922	17.223629	-0.050287	3.150671
259.462355	3282.454306	17.228634	-0.050306	3.147112
259.247294	3274.481665	17.233639	-0.050261	3.143531
259.089701	3266.511929	17.238643	-0.050226	3.139949
259.096384	3258.546460	17.243648	-0.050222	3.136372
259.273737	3250.501911	17.248653	-0.050250	3.132763
259.236523	3242.525689	17.253658	-0.050238	3.129171
259.075939	3234.542366	17.258663	-0.050203	3.125566
258.816051	3226.600234	17.263667	-0.050149	3.121972
258.901837	3218.609144	17.268672	-0.050160	3.118366
258.945513	3210.598293	17.273677	-0.050163	3.114746
258.845411	3202.633014	17.278682	-0.050139	3.111135
258.825843	3194.600215	17.283687	-0.050130	3.107493
258.899693	3186.606071	17.288691	-0.050139	3.103869
258.670967	3178.667822	17.293696	-0.050091	3.100252
258.690111	3170.660049	17.298701	-0.050089	3.096610
258.652749	3162.681037	17.303706	-0.050077	3.092975
258.598275	3154.665920	17.308711	-0.050062	3.089318
258.655209	3146.677175	17.313715	-0.050067	3.085674
258.648158	3138.728166	17.318720	-0.050061	3.082041
258.447337	3130.751444	17.323725	-0.050018	3.078382
258.441693	3122.767348	17.328730	-0.050012	3.074725
258.465094	3114.666008	17.333735	-0.050011	3.071010
258.178323	3106.739726	17.338739	-0.049952	3.067357
258.103137	3098.751346	17.343744	-0.049933	3.063681
258.074923	3090.771210	17.348749	-0.049922	3.060006
258.302493	3082.810509	17.353754	-0.049960	3.056348
257.931909	3074.840466	17.358759	-0.049885	3.052653
257.950830	3066.828962	17.363763	-0.049884	3.048953
258.086283	3058.846946	17.368768	-0.049904	3.045268
257.842011	3050.896649	17.373773	-0.049853	3.041574
257.765459	3042.946968	17.378778	-0.049834	3.037885
257.771627	3034.926549	17.383783	-0.049830	3.034162
257.656876	3026.909657	17.388787	-0.049803	3.030430
257.839557	3018.914855	17.393792	-0.049832	3.026718
257.751549	3010.929686	17.398797	-0.049810	3.022993
257.825454	3002.965022	17.403802	-0.049819	3.019281
257.542090	2995.008525	17.408807	-0.049761	3.015551
257.598690	2986.987910	17.413811	-0.049766	3.011803
257.668208	2979.003888	17.418816	-0.049774	3.008068
257.388927	2971.040935	17.423821	-0.049717	3.004321
257.497139	2963.080035	17.428826	-0.049732	3.000589
257.277496	2955.121574	17.433831	-0.049685	2.996838
257.249152	2947.073521	17.438835	-0.049675	2.993049
257.191217	2939.089116	17.443840	-0.049659	2.989284
257.107760	2931.106253	17.448845	-0.049638	2.985513
257.230364	2923.127583	17.453850	-0.049656	2.981750
257.009578	2915.151103	17.458855	-0.049609	2.977966
256.874458	2907.183033	17.463859	-0.049579	2.974186
256.779990	2899.202422	17.468864	-0.049556	2.970397
256.740879	2891.199208	17.473869	-0.049544	2.966595
256.854648	2883.222117	17.478874	-0.049560	2.962808
256.624324	2875.269013	17.483879	-0.049512	2.959010
256.748235	2867.253609	17.488883	-0.049530	2.955196
256.762865	2859.270675	17.493888	-0.049527	2.951387
256.702760	2851.255148	17.498893	-0.049511	2.947554
256.704101	2843.296281	17.503898	-0.049506	2.943745
256.310388	2835.355166	17.508903	-0.049427	2.939920
256.340003	2827.379496	17.513907	-0.049427	2.936096
256.476548	2819.362358	17.518912	-0.049448	2.932251
256.295457	2811.370006	17.523917	-0.049409	2.928398
256.287866	2803.403105	17.528922	-0.049402	2.924560
256.382063	2795.434292	17.533927	-0.049414	2.920722
256.292669	2787.478481	17.538931	-0.049393	2.916875
256.105082	2779.440706	17.543936	-0.049352	2.912979
255.896262	2771.406446	17.548941	-0.049308	2.909077
255.850806	2763.471983	17.553946	-0.049295	2.905228
255.710300	2755.523157	17.558951	-0.049263	2.901361
255.529543	2747.540015	17.563955	-0.049224	2.897471
255.615233	2739.546658	17.568960	-0.049235	2.893584
255.687222	2731.507905	17.573965	-0.049243	2.889669
255.701980	2723.570707	17.578970	-0.049241	2.885796
255.474403	2715.611008	17.583975	-0.049193	2.881893
255.724273	2707.618783	17.588979	-0.049235	2.877995
255.496252	2699.673836	17.593984	-0.049187	2.874089
255.454270	2691.622466	17.598989	-0.049174	2.870135
255.393130	2683.678305	17.603994	-0.049157	2.866228
255.405102	2675.683585	17.608999	-0.049154	2.862294
255.181354	2667.737638	17.614003	-0.049108	2.858366
255.362135	2659.746616	17.619008	-0.049136	2.854432
255.146697	2651.769359	17.624013	-0.049091	2.850478
255.120883	2643.792034	17.629018	-0.049081	2.846529
255.168797	2635.805518	17.634023	-0.049084	2.842574
255.230979	2627.836653	17.639027	-0.049091	2.838623
255.133275	2619.874962	17.644032	-0.049067	2.834662
254.783103	2611.874073	17.649037	-0.048997	2.830660
254.977923	2603.869147	17.654042	-0.049028	2.826682
254.861798	2595.900740	17.659047	-0.049001	2.822699
254.781963	2587.930769	17.664051	-0.048981	2.818712
254.777919	2579.960978	17.669056	-0.048975	2.814723
254.797183	2571.956246	17.674061	-0.048973	2.810713
254.716618	2563.993006	17.679066	-0.048953	2.806712
254.543287	2556.043735	17.684071	-0.048916	2.802706
254.364384	2548.092306	17.689075	-0.048877	2.798694
254.352364	2540.088609	17.694080	-0.048870	2.794659
254.293155	2532.079049	17.699085	-0.048854	2.790613
254.327529	2524.113533	17.704090	-0.048855	2.786588
254.215179	2516.129640	17.709095	-0.048829	2.782540
254.125377	2508.162814	17.714099	-0.048807	2.778496
254.144340	2500.206690	17.719104	-0.048805	2.774457
254.130806	2492.171426	17.724109	-0.048797	2.770371
254.317027	2484.243009	17.729114	-0.048827	2.766345
254.061667	2476.279649	17.734119	-0.048774	2.762269
253.930402	2468.317964	17.739123	-0.048744	2.758195
254.143502	2460.299757	17.744128	-0.048779	2.754106
253.808835	2452.247916	17.749133	-0.048711	2.749962
253.781361	2444.295781	17.754138	-0.048701	2.745881
253.935097	2436.322027	17.759143	-0.048724	2.741794
253.767947	2428.358465	17.764147	-0.048688	2.737686
253.773247	2420.398708	17.769152	-0.048684	2.733585
253.543789	2412.415167	17.774157	-0.048636	2.729450
253.529223	2404.457643	17.779162	-0.048628	2.725337
253.458966	2396.513320	17.784167	-0.048610	2.721220
253.453526	2388.545678	17.789171	-0.048604	2.717089
253.516950	2380.544110	17.794176	-0.048610	2.712938
253.357545	2372.530911	17.799181	-0.048575	2.708761
253.206863	2364.592611	17.804186	-0.048542	2.704617
253.378267	2356.616094	17.809191	-0.048569	2.700467
253.163573	2348.658562	17.814195	-0.048523	2.696297
253.144008	2340.676943	17.819200	-0.048515	2.692119
253.189872	2332.662359	17.824205	-0.048518	2.687922
253.327318	2324.709869	17.829210	-0.048538	2.683757
252.914471	2316.786118	17.834215	-0.048456	2.679565
252.857244	2308.839183	17.839219	-0.048440	2.675377
252.930741	2300.803731	17.844224	-0.048449	2.671144
252.766627	2292.818606	17.849229	-0.048413	2.666916
252.582019	2284.872900	17.854234	-0.048374	2.662701
252.457903	2276.919578	17.859239	-0.048345	2.658479
252.437228	2268.941099	17.864243	-0.048336	2.654243
252.586227	2260.928567	17.869248	-0.048359	2.649993
252.350264	2252.969643	17.874253	-0.048310	2.645741
252.450024	2245.005706	17.879258	-0.048323	2.641500
252.225018	2237.059812	17.884263	-0.048276	2.637241
252.289469	2229.056683	17.889267	-0.048283	2.632964
252.446044	2221.065388	17.894272	-0.048307	2.628692
252.151490	2213.109662	17.899277	-0.048247	2.624402
252.083287	2205.177223	17.904282	-0.048229	2.620133
252.171872	2197.180178	17.909287	-0.048240	2.615832
252.112282	2189.196908	17.914291	-0.048224	2.611522
252.212363	2181.231039	17.919296	-0.048237	2.607225
252.083351	2173.261979	17.924301	-0.048208	2.602904
251.979142	2165.324725	17.929306	-0.048183	2.598594
251.857330	2157.349458	17.934311	-0.048155	2.594256
251.806389	2149.185781	17.939315	-0.048141	2.589812
251.868211	2141.245072	17.944320	-0.048147	2.585490
251.524063	2133.341765	17.949325	-0.048078	2.581153
251.604957	2125.401298	17.954330	-0.048088	2.576818
251.745445	2117.402868	17.959335	-0.048108	2.572448
251.615563	2109.442794	17.964339	-0.048079	2.568073
251.630812	2101.499963	17.969344	-0.048077	2.563710
251.530509	2093.539572	17.974349	-0.048053	2.559321
251.521051	2085.604625	17.979354	-0.048046	2.554946
251.235480	2077.649819	17.984359	-0.047988	2.550533
251.248982	2069.644604	17.989363	-0.047985	2.546105
251.353925	2061.689553	17.994368	-0.047999	2.541703
251.164945	2053.742820	17.999373	-0.047959	2.537278
251.126165	2045.779748	18.004378	-0.047946	2.532847
251.084285	2037.789313	18.009383	-0.047933	2.528392
250.879114	2029.842746	18.014387	-0.047890	2.523942
250.833553	2021.900807	18.019392	-0.047876	2.519499
250.847816	2013.917911	18.024397	-0.047874	2.515029
250.856859	2005.914283	18.029402	-0.047870	2.510539
250.603060	1997.961179	18.034407	-0.047818	2.506050
250.500337	1990.018575	18.039411	-0.047793	2.501570
250.585664	1982.053892	18.044416	-0.047804	2.497083
250.542104	1974.056878	18.049421	-0.047791	2.492561
250.511401	1966.114061	18.054426	-0.047780	2.488062
250.406276	1958.153997	18.059431	-0.047755	2.483539
250.418068	1950.195826	18.064435	-0.047752	2.479018
250.337552	1942.240840	18.069440	-0.047732	2.474484
250.224429	1934.260686	18.074445	-0.047706	2.469924
250.422714	1926.253744	18.079450	-0.047737	2.465364
250.268326	1918.326487	18.084455	-0.047703	2.460815
250.100249	1910.388298	18.089459	-0.047667	2.456250
250.322505	1902.396607	18.094464	-0.047703	2.451675
250.009287	1894.458848	18.099469	-0.047640	2.447082
249.740667	1886.526555	18.104474	-0.047584	2.442487
249.734474	1878.556835	18.109479	-0.047578	2.437882
249.818594	1870.555553	18.114483	-0.047589	2.433256
249.708843	1862.554873	18.119488	-0.047563	2.428607
249.637086	1854.589793	18.124493	-0.047544	2.423973
249.754190	1846.640771	18.129498	-0.047561	2.419354
249.413320	1838.721665	18.134503	-0.047492	2.414708
249.280913	1830.749593	18.139507	-0.047462	2.410038
249.466315	1822.770624	18.144512	-0.047492	2.405380
249.375663	1814.822369	18.149517	-0.047470	2.400709
249.330751	1806.897346	18.154522	-0.047456	2.396047
249.317687	1798.907280	18.159527	-0.047448	2.391339
249.292994	1790.931591	18.164531	-0.047439	2.386630
249.236591	1782.995927	18.169536	-0.047423	2.381933
249.201188	1775.041028	18.174541	-0.047411	2.377216
249.262291	1767.073772	18.179546	-0.047417	2.372491
249.094734	1759.129153	18.184551	-0.047381	2.367751
248.914110	1751.190262	18.189555	-0.047342	2.363004
248.983358	1743.246356	18.194560	-0.047350	2.358265
248.778761	1735.292978	18.199565	-0.047307	2.353488
248.549129	1727.321547	18.204570	-0.047259	2.348689
248.676927	1719.326052	18.209575	-0.047277	2.343894
248.609592	1711.392640	18.214579	-0.047259	2.339112
248.542642	1703.468977	18.219584	-0.047242	2.334325
248.419406	1695.481296	18.224589	-0.047214	2.329485
248.557525	1687.523418	18.229594	-0.047234	2.324674
248.288532	1679.615213	18.234599	-0.047179	2.319850
248.141317	1671.681919	18.239603	-0.047146	2.315011
248.359126	1663.665880	18.244608	-0.047182	2.310141
248.297208	1655.719097	18.249613	-0.047165	2.305281
248.395564	1647.744765	18.254618	-0.047178	2.300406
248.060711	1639.835689	18.259623	-0.047111	2.295525
247.949708	1631.870840	18.264627	-0.047085	2.290618
247.965611	1623.920866	18.269632	-0.047082	2.285720
247.484614	1616.029522	18.274637	-0.046988	2.280806
247.721876	1608.046699	18.279642	-0.047027	2.275885
247.664036	1599.997748	18.284647	-0.047011	2.270888
247.552346	1592.034939	18.289651	-0.046985	2.265928
247.560980	1584.118028	18.294656	-0.046981	2.260997
247.749193	1576.137041	18.299661	-0.047011	2.256030
247.696725	1568.214860	18.304666	-0.046996	2.251069
247.440794	1560.294929	18.309671	-0.046943	2.246080
247.556687	1552.332334	18.314675	-0.046960	2.241085
247.762713	1544.381765	18.319680	-0.046993	2.236095
247.458644	1536.442415	18.324685	-0.046931	2.231056
247.564954	1528.493425	18.329690	-0.046946	2.226036
247.473148	1520.567873	18.334695	-0.046923	2.221001
247.175663	1512.663895	18.339699	-0.046863	2.215951
247.040612	1504.713489	18.344704	-0.046832	2.210874
246.966469	1496.741612	18.349709	-0.046813	2.205777
247.120928	1488.793550	18.354714	-0.046837	2.200704
246.986637	1480.880556	18.359719	-0.046807	2.195615
246.850635	1472.894811	18.364723	-0.046776	2.190468
246.767478	1464.960850	18.369728	-0.046756	2.185347
246.566369	1457.028913	18.374733	-0.046713	2.180204
246.757079	1449.060550	18.379738	-0.046743	2.175061
246.671304	1441.126082	18.384743	-0.046722	2.169903
246.341218	1433.210007	18.389747	-0.046655	2.164722
246.460334	1425.262354	18.394752	-0.046672	2.159550
246.359984	1417.322690	18.399757	-0.046649	2.154349
246.440096	1409.351055	18.404762	-0.046658	2.149133
246.336729	1401.412804	18.409767	-0.046634	2.143908
246.130496	1393.515303	18.414771	-0.046590	2.138687
246.028350	1385.594916	18.419776	-0.046566	2.133449
245.846998	1377.646976	18.424781	-0.046527	2.128171
245.982299	1369.685845	18.429786	-0.046547	2.122902
245.904343	1361.762837	18.434791	-0.046527	2.117625
245.774813	1353.792223	18.439795	-0.046498	2.112298
245.775021	1345.835213	18.444800	-0.046493	2.106979
245.789756	1337.881987	18.449805	-0.046491	2.101651
245.882462	1329.957351	18.454810	-0.046503	2.096336
245.747304	1322.030161	18.459815	-0.046472	2.090983
245.509859	1314.105397	18.464819	-0.046423	2.085608
245.553208	1306.195462	18.469824	-0.046426	2.080257
245.424769	1298.279578	18.474829	-0.046397	2.074871
245.415841	1290.313098	18.479834	-0.046390	2.069448
245.482843	1282.359617	18.484839	-0.046397	2.064028
245.022026	1274.496004	18.489843	-0.046306	2.058602
245.022191	1266.573822	18.494848	-0.046301	2.053168
244.899055	1258.617423	18.499853	-0.046273	2.047683
245.011323	1250.680248	18.504858	-0.046289	2.042221
244.887045	1242.780640	18.509863	-0.046260	2.036746
244.803422	1234.815209	18.514867	-0.046240	2.031214
244.774299	1226.892648	18.519872	-0.046229	2.025703
244.591406	1218.973374	18.524877	-0.046190	2.020163
244.470895	1211.060497	18.529882	-0.046162	2.014619
244.417583	1203.124859	18.534887	-0.046147	2.009051
244.484933	1195.176764	18.539891	-0.046154	2.003471
244.422586	1187.277675	18.544896	-0.046138	1.997896
244.505785	1179.322186	18.549901	-0.046148	1.992281
244.480402	1171.393934	18.554906	-0.046138	1.986658
244.396567	1163.496370	18.559911	-0.046117	1.981035
244.217423	1155.598941	18.564915	-0.046079	1.975386
244.225360	1147.664293	18.569920	-0.046075	1.969714
244.113781	1139.744430	18.574925	-0.046049	1.964023
244.150329	1131.838891	18.579930	-0.046051	1.958342
243.994809	1123.913431	18.584935	-0.046017	1.952609
243.890778	1115.955147	18.589939	-0.045992	1.946841
243.725268	1108.069470	18.594944	-0.045956	1.941102
243.505202	1100.164434	18.599949	-0.045910	1.935326
243.587820	1092.225461	18.604954	-0.045920	1.929541
243.335378	1084.333816	18.609959	-0.045868	1.923736
243.459250	1076.389484	18.614963	-0.045886	1.917917
243.555466	1068.480074	18.619968	-0.045899	1.912102
243.299525	1060.562808	18.624973	-0.045846	1.906225
243.355481	1052.658908	18.629978	-0.045851	1.900374
243.432063	1044.745109	18.634983	-0.045860	1.894501
243.259006	1036.830083	18.639987	-0.045823	1.888579
243.140022	1028.952409	18.644992	-0.045795	1.882674
243.135756	1021.038657	18.649997	-0.045790	1.876735
242.961877	1013.141382	18.655002	-0.045752	1.870771
242.972567	1005.213398	18.660007	-0.045749	1.864786
242.812859	997.331901	18.665011	-0.045714	1.858797
243.075176	989.391293	18.670016	-0.045758	1.852792
242.895213	981.480698	18.675021	-0.045719	1.846740
242.634051	973.632846	18.680026	-0.045665	1.840706
242.735374	965.724024	18.685031	-0.045679	1.834647
242.553126	957.807457	18.690035	-0.045640	1.828530
242.553173	949.911648	18.695040	-0.045635	1.822429
242.334805	942.037887	18.700045	-0.045589	1.816299
242.465545	934.107371	18.705050	-0.045608	1.810146
242.427480	926.217148	18.710055	-0.045596	1.803983
242.404341	918.336052	18.715059	-0.045586	1.797808
242.514420	910.402894	18.720064	-0.045602	1.791587
242.245958	902.507605	18.725069	-0.045546	1.785327
242.088981	894.654017	18.730074	-0.045512	1.779093
242.134891	886.753564	18.735079	-0.045515	1.772824
242.303720	878.816486	18.740083	-0.045542	1.766519
241.965171	870.997869	18.745088	-0.045474	1.760223
241.798014	863.133598	18.750093	-0.045437	1.753889
241.905552	855.200412	18.755098	-0.045452	1.747511
241.714064	847.349144	18.760103	-0.045411	1.741138
241.439121	839.508907	18.765107	-0.045355	1.734740
241.624558	831.579939	18.770112	-0.045384	1.728305
241.538499	823.704199	18.775117	-0.045363	1.721854
241.253973	815.877602	18.780122	-0.045305	1.715394
241.133325	807.988929	18.785127	-0.045278	1.708880
241.236797	800.064771	18.790131	-0.045292	1.702340
241.347223	792.182195	18.795136	-0.045307	1.695811
241.150172	784.318344	18.800141	-0.045265	1.689231
241.100081	776.450682	18.805146	-0.045251	1.682642
241.174076	768.587327	18.810151	-0.045259	1.676048
240.757316	760.756247	18.815155	-0.045177	1.669388
240.750602	752.883260	18.820160	-0.045170	1.662722
240.810375	744.989263	18.825165	-0.045176	1.656020
240.520486	737.175222	18.830170	-0.045117	1.649311
240.584176	729.284559	18.835175	-0.045124	1.642558
240.526007	721.434420	18.840179	-0.045108	1.635795
240.428705	713.529966	18.845184	-0.045085	1.628951
240.296320	705.671191	18.850189	-0.045055	1.622113
240.189251	697.824950	18.855194	-0.045030	1.615261
240.401774	689.934337	18.860199	-0.045064	1.608385
240.072550	682.131258	18.865203	-0.044998	1.601481
239.977370	674.308828	18.870208	-0.044975	1.594562
240.037744	666.415081	18.875213	-0.044981	1.587573
240.053049	658.561111	18.880218	-0.044979	1.580581
240.100346	650.720798	18.885223	-0.044983	1.573575
239.999421	642.878336	18.890227	-0.044959	1.566515
239.861793	635.087890	18.895232	-0.044928	1.559464
239.555222	627.271943	18.900237	-0.044866	1.552333
239.626393	619.399896	18.905242	-0.044874	1.545173
239.716464	611.569446	18.910247	-0.044886	1.538022
239.473675	603.741665	18.915251	-0.044835	1.530789
239.231365	595.957061	18.920256	-0.044785	1.523562
239.176517	588.130933	18.925261	-0.044770	1.516291
239.118469	580.291243	18.930266	-0.044754	1.508971
238.891128	572.496068	18.935271	-0.044706	1.501631
238.875790	564.661911	18.940275	-0.044698	1.494251
239.026499	556.812096	18.945280	-0.044721	1.486846
238.814940	549.036646	18.950285	-0.044677	1.479417
238.867757	541.191130	18.955290	-0.044682	1.471926
238.732773	533.363847	18.960295	-0.044651	1.464384
238.499989	525.596874	18.965299	-0.044603	1.456846
238.507683	517.784086	18.970304	-0.044599	1.449262
238.556260	509.959880	18.975309	-0.044603	1.441634
238.338570	502.214279	18.980314	-0.044558	1.433999
238.263554	494.409690	18.985319	-0.044538	1.426289
238.430371	486.591026	18.990323	-0.044564	1.418562
238.305852	478.820176	18.995328	-0.044536	1.410792
237.952844	471.083106	19.000333	-0.044465	1.402976
237.788660	463.327637	19.005338	-0.044430	1.395128
237.790861	455.519675	19.010343	-0.044425	1.387211
237.689661	447.748299	19.015347	-0.044401	1.379268
237.792982	439.957036	19.020352	-0.044415	1.371294
237.563702	432.214443	19.025357	-0.044368	1.363266
237.495614	424.466175	19.030362	-0.044350	1.355213
237.696575	416.652848	19.035367	-0.044382	1.347090
237.592721	408.913506	19.040371	-0.044358	1.338942
237.568068	401.173424	19.045376	-0.044348	1.330758
237.440483	393.440196	19.050381	-0.044319	1.322511
237.135935	385.727735	19.055386	-0.044258	1.314204
237.054790	377.877435	19.060391	-0.044237	1.305735
237.019307	370.147789	19.065395	-0.044226	1.297350
236.828369	362.453567	19.070400	-0.044185	1.288921
236.887334	354.715366	19.075405	-0.044191	1.280434
236.666973	347.036933	19.080410	-0.044145	1.271905
236.588526	339.328973	19.085415	-0.044125	1.263312
236.489532	331.630774	19.090419	-0.044102	1.254667
236.478261	323.922235	19.095424	-0.044095	1.245967
236.418487	316.238609	19.100429	-0.044079	1.237225
236.161141	308.565468	19.105434	-0.044026	1.228394
236.169072	300.872137	19.110439	-0.044022	1.219528
235.970522	293.212206	19.115443	-0.043980	1.210595
236.105721	285.512286	19.120448	-0.044000	1.201615
235.814766	277.890627	19.125453	-0.043941	1.192574
235.642775	270.239703	19.130458	-0.043904	1.183453
235.629732	262.588152	19.135463	-0.043897	1.174294
235.500292	254.936103	19.140467	-0.043868	1.165037
235.527224	247.307815	19.145472	-0.043868	1.155768
235.239394	239.654197	19.150477	-0.043809	1.146327
235.087083	232.054433	19.155482	-0.043776	1.136903
235.120818	224.413800	19.160487	-0.043777	1.127388
234.893936	216.839223	19.165491	-0.043730	1.117820
234.923250	209.226861	19.170496	-0.043730	1.108176
234.827022	201.636686	19.175501	-0.043707	1.098449
234.647234	194.072605	19.180506	-0.043669	1.088650
234.566859	186.511471	19.185511	-0.043649	1.078789
234.141737	178.988651	19.190515	-0.043565	1.068808
234.154887	171.421089	19.195520	-0.043563	1.058774
233.961525	163.887869	19.200525	-0.043522	1.048642
233.742599	156.383427	19.205530	-0.043476	1.038445
233.479176	148.889792	19.210535	-0.043422	1.028150
233.068017	141.427032	19.215539	-0.043341	1.017759
232.622499	133.982854	19.220544	-0.043253	1.007277
232.290312	126.532379	19.225549	-0.043186	0.996704
231.949367	119.046386	19.230554	-0.043118	0.985965
231.494638	111.636799	19.235559	-0.043028	0.975189
231.016304	104.227120	19.240563	-0.042934	0.964286
230.661633	96.834129	19.245568	-0.042863	0.953315
230.040648	89.477341	19.250573	-0.042743	0.942201
229.557850	82.119365	19.255578	-0.042648	0.930988
229.180460	74.761544	19.260583	-0.042573	0.919667
228.798803	67.402807	19.265587	-0.042497	0.908202
228.167805	60.350497	19.270592	-0.042375	0.897003