Tue Mar 23 10:51:40 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.650437	-0.049021	0.000000	-0.000048	0.722079

0.633328	-0.044587	0.005005	-0.000045	0.722081
0.761693	-0.074989	0.010010	-0.000069	0.722067
0.844087	-0.083225	0.015014	-0.000084	0.722079
0.599156	-0.042722	0.020019	-0.000039	0.722073
0.525328	-0.057066	0.025024	-0.000025	0.722019
0.741045	-0.235211	0.030029	-0.000065	0.721745
0.413403	-0.178234	0.035034	-0.000004	0.721742
0.580534	-0.202829	0.040038	-0.000036	0.721753
0.533182	-0.197181	0.045043	-0.000027	0.721747
0.680561	-0.223938	0.050048	-0.000054	0.721746
0.783164	-0.239785	0.055053	-0.000073	0.721751
0.670506	-0.224853	0.060058	-0.000052	0.721741
0.420779	-0.173568	0.065062	-0.000006	0.721755
0.269822	-0.148442	0.070067	0.000022	0.721751
0.489550	-0.193717	0.075072	-0.000019	0.721739
0.545523	-0.350512	0.080077	-0.000029	0.721451
0.627763	-0.371744	0.085082	-0.000045	0.721438
0.482667	-0.341390	0.090086	-0.000018	0.721447
0.583745	-0.363000	0.095091	-0.000037	0.721440
0.572278	-0.361358	0.100096	-0.000034	0.721439
0.506987	-0.347554	0.105101	-0.000022	0.721443
0.285855	-0.466497	0.110106	0.000019	0.721132
0.581211	-0.520037	0.115110	-0.000036	0.721130
0.516639	-0.512232	0.120115	-0.000024	0.721123
0.459592	-0.500690	0.125120	-0.000014	0.721126
0.528287	-0.518120	0.130125	-0.000026	0.721116
0.271542	-0.592108	0.135130	0.000021	0.720880
0.438758	-0.618630	0.140134	-0.000010	0.720887
0.365348	-0.607308	0.145139	0.000004	0.720883
0.450734	-0.621601	0.150144	-0.000012	0.720885
0.501507	-0.772144	0.155149	-0.000021	0.720607
0.683127	-0.840989	0.160154	-0.000055	0.720535
0.702369	-0.839543	0.165158	-0.000059	0.720545
0.618907	-0.877398	0.170163	-0.000043	0.720441
0.304753	-0.932295	0.175168	0.000015	0.720223
0.389244	-0.946271	0.180173	-0.000001	0.720225
0.290720	-0.930515	0.185178	0.000018	0.720221
0.184497	-1.054875	0.190182	0.000037	0.719939
-0.062214	-1.025365	0.195187	0.000083	0.719911
0.064313	-1.051856	0.200192	0.000060	0.719903
-0.056248	-1.116038	0.205197	0.000082	0.719734
0.068546	-1.206984	0.210202	0.000059	0.719599
0.159927	-1.217162	0.215206	0.000042	0.719611
0.161098	-1.311849	0.220211	0.000042	0.719425
0.301738	-1.417458	0.225216	0.000016	0.719266
0.444844	-1.437997	0.230221	-0.000011	0.719276
0.155485	-1.522241	0.235226	0.000043	0.719008
0.122576	-1.534775	0.240230	0.000049	0.718972
0.174433	-1.579525	0.245235	0.000039	0.718902
0.309112	-1.731693	0.250240	0.000014	0.718649
0.148226	-1.700834	0.255245	0.000044	0.718653
-0.099569	-1.764775	0.260250	0.000090	0.718440
-0.069091	-1.806403	0.265254	0.000084	0.718369
-0.153932	-1.837608	0.270259	0.000100	0.718277
-0.464928	-1.910419	0.275264	0.000158	0.718024
-0.315160	-1.933300	0.280269	0.000130	0.718031
-0.292130	-2.068984	0.285274	0.000126	0.717772
-0.364541	-2.084045	0.290278	0.000139	0.717716
-0.378745	-2.157035	0.295283	0.000142	0.717567
-0.135308	-2.291361	0.300288	0.000097	0.717387
-0.344050	-2.288875	0.305293	0.000136	0.717319
-0.737726	-2.336373	0.310298	0.000209	0.717086
-1.006314	-2.281878	0.315302	0.000259	0.717099
-2.839938	-2.115004	0.320307	0.000600	0.716783
-2.725141	-2.147358	0.325312	0.000579	0.716760
-2.720961	-2.144597	0.330317	0.000578	0.716767
-3.578005	-2.140999	0.335322	0.000737	0.716472
-3.636587	-2.136953	0.340326	0.000748	0.716459
-3.866269	-2.099873	0.345331	0.000791	0.716452
-3.614899	-2.236214	0.350336	0.000744	0.716271
-4.693603	-2.110241	0.355341	0.000945	0.716140
-4.485715	-2.152310	0.360346	0.000906	0.716130
-4.343152	-2.173962	0.365350	0.000880	0.716137
-5.175255	-2.147771	0.370355	0.001035	0.715895
-5.295626	-2.132753	0.375360	0.001057	0.715883
-5.064139	-2.173079	0.380365	0.001014	0.715885
-5.475350	-2.102876	0.385370	0.001090	0.715879
-6.066177	-2.161720	0.390374	0.001200	0.715554
-6.215069	-2.138943	0.395379	0.001228	0.715546
-6.488339	-2.088582	0.400384	0.001279	0.715550
-6.176890	-2.141499	0.405389	0.001221	0.715555
-6.452248	-2.170923	0.410394	0.001272	0.715399
-7.374580	-2.086276	0.415398	0.001444	0.715241
-7.108231	-2.137574	0.420403	0.001394	0.715234
-7.425534	-2.079606	0.425408	0.001453	0.715237
-7.071022	-2.142595	0.430413	0.001387	0.715237
-7.391778	-2.182537	0.435418	0.001447	0.715045
-8.578230	-2.038769	0.440422	0.001667	0.714911
-8.216607	-2.105936	0.445427	0.001600	0.714905
-8.111464	-2.123998	0.450432	0.001581	0.714907
-8.433910	-2.061968	0.455437	0.001640	0.714916
-8.403086	-2.070567	0.460442	0.001635	0.714910
-8.289957	-2.207003	0.465446	0.001614	0.714679
-9.248260	-2.071922	0.470451	0.001792	0.714608
-9.143182	-2.092135	0.475456	0.001772	0.714605
-8.676760	-2.170305	0.480461	0.001686	0.714615
-9.384783	-2.050286	0.485466	0.001817	0.714603
-9.103617	-2.095379	0.490470	0.001765	0.714613
-9.375563	-2.215424	0.495475	0.001816	0.714279
-9.798023	-2.139705	0.500480	0.001894	0.714280
-10.162530	-2.073956	0.505485	0.001962	0.714281
-9.947292	-2.117365	0.510490	0.001922	0.714271
-9.903451	-2.120150	0.515494	0.001914	0.714281
-10.069904	-2.091171	0.520499	0.001945	0.714280
-10.602241	-2.131021	0.525504	0.002044	0.714013
-10.822525	-2.107727	0.530509	0.002085	0.713981
-11.299853	-2.027613	0.535514	0.002173	0.713971
-10.728672	-2.127710	0.540518	0.002067	0.713975
-10.877269	-2.105052	0.545523	0.002095	0.713967
-10.984304	-2.085440	0.550528	0.002115	0.713968
-10.993781	-2.105820	0.555533	0.002116	0.713925
-11.948366	-2.074620	0.560538	0.002294	0.713649
-11.428883	-2.164099	0.565542	0.002197	0.713655
-11.858517	-2.089454	0.570547	0.002277	0.713651
-12.036352	-2.058917	0.575552	0.002310	0.713649
-11.549787	-2.141904	0.580557	0.002220	0.713656
-11.958181	-2.073672	0.585562	0.002296	0.713647
-11.771427	-2.174123	0.590566	0.002261	0.713514
-12.754239	-2.077127	0.595571	0.002444	0.713359
-12.528440	-2.117745	0.600576	0.002402	0.713358
-12.556628	-2.109157	0.605581	0.002407	0.713365
-12.898519	-2.053749	0.610586	0.002470	0.713354
-12.423841	-2.134073	0.615590	0.002382	0.713363
-12.654033	-2.096209	0.620595	0.002425	0.713357
-13.292633	-2.103608	0.625600	0.002544	0.713116
-13.624099	-2.089657	0.630605	0.002605	0.713026
-13.736369	-2.072405	0.635610	0.002626	0.713021
-13.768533	-2.061974	0.640614	0.002632	0.713030
-13.889602	-2.041154	0.645619	0.002655	0.713029
-13.712749	-2.073956	0.650624	0.002622	0.713026
-13.581397	-2.094222	0.655629	0.002597	0.713032
-13.965103	-2.059393	0.660634	0.002669	0.712966
-14.317017	-2.121278	0.665638	0.002734	0.712718
-14.372117	-2.114993	0.670643	0.002744	0.712711
-14.947558	-2.012367	0.675648	0.002851	0.712711
-14.385706	-2.108150	0.680653	0.002747	0.712720
-14.560594	-2.083308	0.685658	0.002779	0.712707
-14.741452	-2.047996	0.690662	0.002813	0.712714
-14.765352	-2.045388	0.695667	0.002817	0.712710
-15.252769	-2.120849	0.700672	0.002908	0.712387
-15.490394	-2.074720	0.705677	0.002952	0.712395
-15.778715	-2.029823	0.710682	0.003006	0.712382
-15.189301	-2.129932	0.715686	0.002896	0.712392
-15.622494	-2.055701	0.720691	0.002977	0.712386
-15.907744	-2.005945	0.725696	0.003030	0.712384
-15.625554	-2.051676	0.730701	0.002977	0.712393
-15.793353	-2.104900	0.735706	0.003008	0.712228
-16.823491	-1.988658	0.740710	0.003200	0.712094
-16.329874	-2.076521	0.745715	0.003108	0.712094
-16.337996	-2.076957	0.750720	0.003110	0.712090
-16.408423	-2.063826	0.755725	0.003123	0.712091
-16.593978	-2.033748	0.760730	0.003157	0.712086
-16.336034	-2.076181	0.765734	0.003109	0.712093
-16.330934	-2.129400	0.770739	0.003108	0.711988
-17.785630	-1.984773	0.775744	0.003379	0.711760
-17.175134	-2.090135	0.780749	0.003265	0.711767
-17.481869	-2.039679	0.785754	0.003322	0.711759
-17.582695	-2.018158	0.790758	0.003341	0.711766
-17.485555	-2.039381	0.795763	0.003323	0.711758
-17.427428	-2.051032	0.800768	0.003312	0.711756
-17.314709	-2.065677	0.805773	0.003291	0.711767
-18.045531	-2.055332	0.810778	0.003427	0.711528
-18.304193	-2.042856	0.815782	0.003475	0.711461
-18.245875	-2.053875	0.820787	0.003464	0.711460
-18.575465	-1.997897	0.825792	0.003526	0.711454
-18.573539	-1.992924	0.830797	0.003525	0.711465
-18.207931	-2.063892	0.835802	0.003457	0.711453
-18.095075	-2.081381	0.840806	0.003436	0.711459
-18.600236	-2.038402	0.845811	0.003530	0.711365
-19.469461	-1.997771	0.850816	0.003692	0.711137
-18.915337	-2.093684	0.855821	0.003589	0.711143
-19.491430	-1.996444	0.860826	0.003696	0.711132
-19.260719	-2.034307	0.865830	0.003653	0.711138
-18.985724	-2.084555	0.870835	0.003602	0.711136
-19.678127	-1.962409	0.875840	0.003730	0.711134
-19.130849	-2.055929	0.880845	0.003628	0.711142
-19.261391	-2.163558	0.885850	0.003653	0.710881
-19.887213	-2.054757	0.890854	0.003769	0.710875
-20.242577	-1.994573	0.895859	0.003835	0.710869
-19.983155	-2.039976	0.900864	0.003787	0.710871
-19.622519	-2.100442	0.905869	0.003720	0.710878
-20.086458	-2.022594	0.910874	0.003806	0.710869
-19.963297	-2.108984	0.915878	0.003783	0.710740
-20.592686	-2.100310	0.920883	0.003900	0.710534
-20.669234	-2.088589	0.925888	0.003915	0.710530
-20.780632	-2.063236	0.930893	0.003935	0.710541
-20.895383	-2.048107	0.935898	0.003957	0.710530
-20.640490	-2.089775	0.940902	0.003909	0.710538
-20.786125	-2.062854	0.945907	0.003936	0.710540
-21.508350	-2.065372	0.950912	0.004071	0.710278
-21.294047	-2.129878	0.955917	0.004031	0.710225
-21.787932	-2.047193	0.960922	0.004123	0.710215
-21.712086	-2.057469	0.965926	0.004108	0.710221
-21.518921	-2.092085	0.970931	0.004072	0.710221
-21.659309	-2.067114	0.975936	0.004098	0.710221
-21.629067	-2.071412	0.980941	0.004093	0.710223
-22.363458	-2.105850	0.985946	0.004230	0.709893
-22.337473	-2.107244	0.990950	0.004225	0.709900
-22.858819	-2.014511	0.995955	0.004322	0.709899
-22.659635	-2.052073	1.000960	0.004284	0.709895
-22.301029	-2.113358	1.005965	0.004218	0.709901
-22.971732	-1.999046	1.010970	0.004342	0.709890
-22.727183	-2.036183	1.015974	0.004297	0.709903
-22.782690	-2.146524	1.020979	0.004307	0.709663
-23.629910	-2.030523	1.025984	0.004465	0.709593
-23.416698	-2.063992	1.030989	0.004425	0.709602
-23.469326	-2.058245	1.035994	0.004435	0.709595
-23.425593	-2.063076	1.040998	0.004427	0.709601
-23.486051	-2.052853	1.046003	0.004438	0.709600
-23.773102	-2.004128	1.051008	0.004491	0.709595
-23.697305	-2.143580	1.056013	0.004477	0.709343
-24.441408	-2.052056	1.061018	0.004616	0.709261
-24.396385	-2.057625	1.066022	0.004607	0.709266
-24.476278	-2.043782	1.071027	0.004622	0.709265
-24.725139	-2.001547	1.076032	0.004668	0.709261
-24.323658	-2.069035	1.081037	0.004594	0.709270
-24.391657	-2.061795	1.086042	0.004606	0.709260
-24.629359	-2.115310	1.091046	0.004650	0.709068
-25.630882	-1.993213	1.096051	0.004837	0.708955
-25.372899	-2.041876	1.101056	0.004789	0.708950
-25.169846	-2.072411	1.106061	0.004751	0.708961
-25.635968	-1.992980	1.111066	0.004838	0.708954
-25.588313	-1.996486	1.116070	0.004829	0.708964
-25.274454	-2.054131	1.121075	0.004770	0.708961
-25.383551	-2.069614	1.126080	0.004791	0.708891
-26.073535	-2.071544	1.131085	0.004919	0.708641
-26.276313	-2.037595	1.136090	0.004957	0.708637
-26.573364	-1.980770	1.141094	0.005012	0.708644
-26.001791	-2.085313	1.146099	0.004906	0.708639
-26.254845	-2.041742	1.151104	0.004953	0.708636
-26.309577	-2.028136	1.156109	0.004963	0.708644
-26.253727	-2.041208	1.161114	0.004952	0.708638
-26.765019	-2.084394	1.166118	0.005047	0.708369
-26.981130	-2.053753	1.171123	0.005088	0.708353
-27.209644	-2.014554	1.176128	0.005130	0.708350
-26.727769	-2.097273	1.181133	0.005040	0.708357
-27.165940	-2.023673	1.186138	0.005122	0.708348
-26.863682	-2.074111	1.191142	0.005066	0.708355
-26.891510	-2.106964	1.196147	0.005071	0.708279
-28.137034	-2.019781	1.201152	0.005303	0.708009
-27.849524	-2.066855	1.206157	0.005249	0.708017
-28.231908	-2.003114	1.211162	0.005320	0.708008
-28.175760	-2.010593	1.216166	0.005310	0.708014
-27.914278	-2.058984	1.221171	0.005261	0.708010
-28.153261	-2.018891	1.226176	0.005305	0.708005
-28.191682	-2.005976	1.231181	0.005312	0.708017
-28.468855	-2.075310	1.236186	0.005364	0.707779
-29.183821	-1.986923	1.241190	0.005497	0.707701
-29.005908	-2.016570	1.246195	0.005464	0.707705
-29.021989	-2.017598	1.251200	0.005467	0.707698
-28.899921	-2.035231	1.256205	0.005444	0.707706
-28.786209	-2.059467	1.261210	0.005423	0.707698
-28.991919	-2.019621	1.266214	0.005461	0.707705
-28.986489	-2.088625	1.271219	0.005460	0.707568
-30.114838	-1.984612	1.276224	0.005670	0.707373
-29.492580	-2.090376	1.281229	0.005554	0.707384
-29.908000	-2.021713	1.286234	0.005632	0.707373
-29.950445	-2.010147	1.291238	0.005639	0.707381
-29.669775	-2.059547	1.296243	0.005587	0.707383
-29.990879	-2.005670	1.301248	0.005647	0.707376
-29.860751	-2.071127	1.306253	0.005623	0.707291
-30.624074	-2.039235	1.311258	0.005765	0.707082
-30.627855	-2.034601	1.316262	0.005765	0.707090
-30.817072	-2.001777	1.321267	0.005801	0.707088
-30.503523	-2.061352	1.326272	0.005742	0.707081
-30.415216	-2.071224	1.331277	0.005726	0.707093
-30.740559	-2.017638	1.336282	0.005786	0.707084
-30.728331	-2.092183	1.341286	0.005784	0.706939
-31.530017	-2.040188	1.346291	0.005933	0.706757
-31.776351	-1.997495	1.351296	0.005979	0.706754
-31.538666	-2.035779	1.356301	0.005935	0.706762
-31.553707	-2.038308	1.361306	0.005937	0.706752
-31.498065	-2.046363	1.366310	0.005927	0.706756
-31.710280	-2.006176	1.371315	0.005966	0.706761
-31.790219	-2.031438	1.376320	0.005981	0.706681
-32.230161	-2.066787	1.381325	0.006063	0.706453
-32.517644	-2.020875	1.386330	0.006117	0.706442
-32.654446	-1.995177	1.391334	0.006142	0.706445
-32.226585	-2.070386	1.396339	0.006062	0.706447
-32.733151	-1.983603	1.401344	0.006157	0.706440
-32.489181	-2.023904	1.406349	0.006111	0.706447
-32.483892	-2.046749	1.411354	0.006110	0.706403
-33.085753	-2.077333	1.416358	0.006222	0.706126
-33.260773	-2.043620	1.421363	0.006255	0.706131
-33.742798	-1.963186	1.426368	0.006344	0.706120
-33.099093	-2.072133	1.431373	0.006225	0.706132
-33.635601	-1.981368	1.436378	0.006324	0.706122
-33.472856	-2.009173	1.441382	0.006294	0.706124
-32.899176	-2.122638	1.446387	0.006187	0.706102
-34.046676	-2.039229	1.451392	0.006401	0.705858
-34.207974	-2.006566	1.456397	0.006431	0.705866
-34.072679	-2.035339	1.461402	0.006406	0.705857
-33.931210	-2.057685	1.466406	0.006379	0.705863
-33.984179	-2.048248	1.471411	0.006389	0.705863
-34.141367	-2.024116	1.476416	0.006418	0.705855
-33.897631	-2.150108	1.481421	0.006373	0.705689
-35.375949	-1.972487	1.486426	0.006648	0.705517
-34.861376	-2.062383	1.491430	0.006552	0.705520
-34.460440	-2.132994	1.496435	0.006477	0.705522
-35.254516	-1.994801	1.501440	0.006625	0.705516
-34.943659	-2.045247	1.506445	0.006567	0.705526
-34.788468	-2.077370	1.511450	0.006538	0.705517
-35.167259	-2.138843	1.516454	0.006609	0.705257
-35.767460	-2.057024	1.521459	0.006721	0.705207
-35.977544	-2.022179	1.526464	0.006760	0.705201
-35.371732	-2.125239	1.531469	0.006647	0.705211
-35.801568	-2.052002	1.536474	0.006727	0.705205
-35.935522	-2.026812	1.541478	0.006752	0.705207
-35.700027	-2.102508	1.546483	0.006708	0.705140
-36.806441	-2.034215	1.551488	0.006914	0.704880
-36.415776	-2.100868	1.556493	0.006841	0.704886
-36.605555	-2.069060	1.561498	0.006876	0.704882
-36.489107	-2.087456	1.566502	0.006855	0.704887
-36.655175	-2.056968	1.571507	0.006885	0.704889
-36.882118	-2.019194	1.576512	0.006928	0.704883
-36.308190	-2.185799	1.581517	0.006821	0.704754
-37.904980	-1.984679	1.586522	0.007118	0.704586
-37.616747	-2.033697	1.591526	0.007064	0.704591
-37.312063	-2.087738	1.596531	0.007008	0.704591
-37.892894	-1.983321	1.601536	0.007116	0.704593
-37.539849	-2.046447	1.606541	0.007050	0.704593
-37.630334	-2.033381	1.611546	0.007067	0.704587
-37.375054	-2.143277	1.616550	0.007019	0.704457
-38.588488	-2.023568	1.621555	0.007245	0.704262
-38.696250	-2.007731	1.626560	0.007265	0.704256
-38.283980	-2.075532	1.631565	0.007188	0.704267
-38.654937	-2.011077	1.636570	0.007257	0.704264
-38.805028	-1.983398	1.641574	0.007285	0.704266
-38.531728	-2.031498	1.646579	0.007234	0.704267
-38.564259	-2.034257	1.651584	0.007240	0.704250
-38.906367	-2.117843	1.656589	0.007304	0.703959
-39.319227	-2.047425	1.661594	0.007381	0.703952
-39.440754	-2.025495	1.666598	0.007403	0.703953
-39.197999	-2.068655	1.671603	0.007358	0.703953
-39.420709	-2.032442	1.676608	0.007399	0.703946
-39.180474	-2.070355	1.681613	0.007355	0.703956
-39.523120	-2.033923	1.686618	0.007418	0.703907
-40.077388	-2.070218	1.691622	0.007522	0.703634
-39.915828	-2.097513	1.696627	0.007491	0.703637
-40.273570	-2.037034	1.701632	0.007558	0.703631
-40.094115	-2.064696	1.706637	0.007525	0.703639
-40.508975	-1.993261	1.711642	0.007602	0.703634
-40.386226	-2.017350	1.716646	0.007579	0.703630
-40.184684	-2.071762	1.721651	0.007541	0.703593
-41.193842	-2.019445	1.726656	0.007729	0.703335
-40.780374	-2.087201	1.731661	0.007652	0.703347
-41.243569	-2.008694	1.736666	0.007738	0.703339
-41.116676	-2.030313	1.741670	0.007715	0.703341
-40.896241	-2.069766	1.746675	0.007674	0.703341
-41.369083	-1.986833	1.751680	0.007761	0.703338
-41.141029	-2.044728	1.756685	0.007719	0.703304
-41.854288	-2.068627	1.761690	0.007852	0.702999
-41.664833	-2.098927	1.766694	0.007817	0.703006
-42.089656	-2.024320	1.771699	0.007896	0.703004
-42.161595	-2.014242	1.776704	0.007909	0.702998
-41.708641	-2.090781	1.781709	0.007825	0.703007
-42.046388	-2.034942	1.786714	0.007887	0.702998
-42.106233	-2.052052	1.791718	0.007898	0.702942
-42.832308	-2.047402	1.796723	0.008034	0.702690
-42.821156	-2.051402	1.801728	0.008031	0.702686
-42.586561	-2.089945	1.806733	0.007988	0.702693
-42.819712	-2.050509	1.811738	0.008031	0.702688
-42.754282	-2.060285	1.816742	0.008019	0.702692
-42.774508	-2.056992	1.821747	0.008023	0.702692
-42.751077	-2.115420	1.826752	0.008018	0.702582
-43.632305	-2.062588	1.831757	0.008182	0.702371
-43.434408	-2.101924	1.836762	0.008145	0.702363
-43.982920	-2.002136	1.841766	0.008247	0.702367
-43.737747	-2.044496	1.846771	0.008202	0.702370
-43.844850	-2.028070	1.851776	0.008222	0.702365
-43.873383	-2.019397	1.856781	0.008227	0.702372
-44.011611	-2.010659	1.861786	0.008253	0.702340
-44.437380	-2.066413	1.866790	0.008332	0.702074
-44.197197	-2.109120	1.871795	0.008287	0.702074
-44.886141	-1.989117	1.876800	0.008415	0.702069
-44.538082	-2.047160	1.881805	0.008350	0.702077
-44.635444	-2.033741	1.886810	0.008369	0.702069
-44.681356	-2.023515	1.891814	0.008377	0.702073
-44.455500	-2.101820	1.896819	0.008335	0.701996
-45.485637	-2.045478	1.901824	0.008527	0.701739
-45.138147	-2.103847	1.906829	0.008462	0.701746
-45.615281	-2.019018	1.911834	0.008551	0.701746
-45.565298	-2.025233	1.916838	0.008541	0.701751
-45.221095	-2.085522	1.921843	0.008477	0.701754
-45.651900	-2.013388	1.926848	0.008557	0.701744
-45.324403	-2.116349	1.931853	0.008496	0.701654
-46.203272	-2.068138	1.936858	0.008660	0.701434
-46.160900	-2.075080	1.941862	0.008652	0.701436
-46.268039	-2.051126	1.946867	0.008672	0.701446
-46.370424	-2.034302	1.951872	0.008691	0.701443
-46.360038	-2.027023	1.956877	0.008689	0.701461
-46.896924	-1.936859	1.961882	0.008789	0.701450
-46.506111	-2.047699	1.966886	0.008716	0.701367
-47.018674	-2.074723	1.971891	0.008812	0.701127
-47.130535	-2.058212	1.976896	0.008832	0.701120
-47.320578	-2.017399	1.981901	0.008868	0.701135
-47.051971	-2.071225	1.986906	0.008818	0.701123
-47.240652	-2.036048	1.991910	0.008853	0.701126
-47.223001	-2.038429	1.996915	0.008849	0.701127
-47.333438	-2.095070	2.001920	0.008870	0.700973

-48.024140	-2.018128	2.011917	0.008998	0.700879
-47.939486	-2.031262	2.021914	0.008983	0.700883
-48.011426	-2.020911	2.031910	0.008996	0.700879
-48.046327	-2.014503	2.041907	0.009002	0.700879
-47.718251	-2.073428	2.051904	0.008941	0.700878
-48.105674	-2.003667	2.061901	0.009013	0.700880
-47.794393	-2.062875	2.071898	0.008955	0.700873
-47.926010	-2.039841	2.081894	0.008980	0.700872
-47.992135	-2.027095	2.091891	0.008992	0.700874
-47.818960	-2.057554	2.101888	0.008959	0.700875
-48.277554	-1.977340	2.111885	0.009045	0.700872
-47.860538	-2.051660	2.121882	0.008967	0.700872
-47.488599	-2.003058	2.131878	0.008898	0.701105
-46.972591	-2.088430	2.141875	0.008801	0.701119
-47.216385	-2.043815	2.151872	0.008847	0.701122
-47.457788	-1.996501	2.161869	0.008892	0.701130
-47.387018	-2.001874	2.171866	0.008878	0.701145
-46.496396	-2.015137	2.181862	0.008712	0.701440
-46.242366	-2.059315	2.191859	0.008665	0.701443
-46.407808	-2.029016	2.201856	0.008696	0.701444
-46.442167	-2.027220	2.211853	0.008702	0.701436
-45.555263	-2.051952	2.221850	0.008537	0.701706
-45.681394	-2.010054	2.231846	0.008560	0.701745
-45.374519	-2.062841	2.241843	0.008503	0.701750
-45.313112	-2.074298	2.251840	0.008492	0.701749
-44.896147	-2.014296	2.261837	0.008414	0.702021
-44.603471	-2.039597	2.271834	0.008359	0.702075
-44.538400	-2.050587	2.281830	0.008347	0.702077
-44.423095	-2.070803	2.291827	0.008325	0.702078
-44.091402	-1.982084	2.301824	0.008264	0.702377
-43.744923	-2.044245	2.311821	0.008199	0.702376
-43.789832	-2.035744	2.321818	0.008207	0.702377
-43.622968	-1.983176	2.331814	0.008176	0.702544
-43.011385	-2.015744	2.341811	0.008062	0.702699
-43.182660	-1.986417	2.351808	0.008094	0.702696
-43.074208	-1.965546	2.361805	0.008074	0.702778
-42.131269	-2.019289	2.371802	0.007898	0.703009
-42.184284	-2.009652	2.381798	0.007908	0.703010
-41.996534	-2.043051	2.391795	0.007873	0.703010
-41.718250	-1.956443	2.401792	0.007821	0.703285
-41.214427	-2.018477	2.411789	0.007727	0.703342
-41.116278	-2.035091	2.421786	0.007709	0.703344
-41.070418	-2.003835	2.431782	0.007700	0.703423
-40.160041	-2.057230	2.441779	0.007530	0.703643
-40.508549	-1.993139	2.451776	0.007595	0.703647
-40.490823	-1.999519	2.461773	0.007592	0.703641
-39.801081	-1.992246	2.471770	0.007463	0.703904
-39.732240	-1.975783	2.481766	0.007450	0.703962
-39.549245	-2.010773	2.491763	0.007416	0.703958
-39.448438	-1.948131	2.501760	0.007397	0.704120
-38.659626	-2.015548	2.511757	0.007250	0.704268
-38.816630	-1.989119	2.521754	0.007279	0.704265
-38.776768	-1.971274	2.531750	0.007272	0.704316
-37.690003	-2.027614	2.541747	0.007069	0.704593
-37.805618	-2.004532	2.551744	0.007091	0.704598
-37.888989	-1.989795	2.561741	0.007106	0.704598
-37.537639	-1.955832	2.571738	0.007041	0.704793
-36.933860	-2.012997	2.581734	0.006928	0.704895
-37.136334	-1.976372	2.591731	0.006966	0.704896
-37.067411	-1.947661	2.601728	0.006953	0.704979
-36.113556	-1.999533	2.611725	0.006775	0.705217
-36.229654	-1.978149	2.621722	0.006797	0.705218
-36.058326	-2.009508	2.631718	0.006765	0.705217
-35.131140	-2.045944	2.641715	0.006592	0.705476
-35.488615	-1.955797	2.651712	0.006659	0.705530
-35.096663	-2.021975	2.661709	0.006586	0.705537
-35.463247	-1.901001	2.671706	0.006654	0.705649
-34.158253	-2.019994	2.681702	0.006411	0.705878
-34.552773	-1.949103	2.691699	0.006484	0.705879
-34.562486	-1.948816	2.701696	0.006486	0.705877
-33.717771	-1.973568	2.711693	0.006328	0.706130
-33.650403	-1.980608	2.721690	0.006316	0.706140
-33.723988	-1.962137	2.731686	0.006329	0.706151
-33.244418	-1.947687	2.741683	0.006240	0.706352
-32.617533	-2.012962	2.751680	0.006123	0.706446
-32.679130	-2.002147	2.761677	0.006134	0.706446
-32.881281	-1.936110	2.771674	0.006172	0.706506
-31.869346	-1.986767	2.781670	0.005984	0.706767
-31.993885	-1.964073	2.791667	0.006007	0.706768
-31.987380	-1.963916	2.801664	0.006005	0.706771
-31.404420	-1.922464	2.811661	0.005897	0.707063
-31.044191	-1.971025	2.821658	0.005830	0.707094
-30.976850	-1.981360	2.831654	0.005817	0.707098
-31.016769	-1.888276	2.841651	0.005824	0.707271
-30.307530	-1.951221	2.851648	0.005692	0.707398
-30.143429	-1.988026	2.861645	0.005661	0.707383
-30.150616	-1.959848	2.871642	0.005663	0.707437
-29.172266	-2.000745	2.881638	0.005480	0.707705
-29.180389	-2.000317	2.891635	0.005482	0.707704
-29.268735	-1.983450	2.901632	0.005498	0.707706
-29.082225	-1.922691	2.911629	0.005463	0.707895
-28.518777	-1.957371	2.921626	0.005358	0.708027
-28.504621	-1.961342	2.931622	0.005356	0.708024
-28.261918	-1.973110	2.941619	0.005310	0.708087
-27.223061	-2.021455	2.951616	0.005117	0.708362
-27.391956	-1.993782	2.961613	0.005148	0.708357
-27.373938	-2.000392	2.971610	0.005145	0.708350
-27.435675	-1.927009	2.981606	0.005156	0.708476
-26.537417	-2.000851	2.991603	0.004989	0.708648
-26.936319	-1.920999	3.001600	0.005063	0.708666
-27.069014	-1.871849	3.011597	0.005088	0.708717
-25.870327	-1.960443	3.021594	0.004864	0.708968
-25.930729	-1.945472	3.031590	0.004876	0.708977
-25.959032	-1.942699	3.041587	0.004881	0.708972
-25.056182	-1.973841	3.051584	0.004713	0.709232
-24.946856	-1.975057	3.061581	0.004692	0.709269
-24.776021	-2.006910	3.071578	0.004660	0.709266
-24.951390	-1.934125	3.081574	0.004693	0.709350
-24.131925	-1.953732	3.091571	0.004540	0.709603
-23.903851	-1.992503	3.101568	0.004498	0.709607
-24.037830	-1.970902	3.111565	0.004522	0.709602
-23.347552	-1.997565	3.121562	0.004394	0.709795
-23.147226	-1.981687	3.131558	0.004356	0.709898
-22.934253	-2.020774	3.141555	0.004317	0.709896
-22.970610	-2.015084	3.151552	0.004323	0.709895
-22.406509	-1.963592	3.161549	0.004218	0.710199
-22.029455	-2.019091	3.171546	0.004148	0.710222
-22.133839	-2.001828	3.181542	0.004167	0.710220
-22.022869	-1.974257	3.191539	0.004146	0.710315
-21.121107	-2.023591	3.201536	0.003979	0.710537
-21.206109	-2.010017	3.211533	0.003994	0.710534
-21.260966	-2.000484	3.221530	0.004004	0.710534
-20.762215	-1.981066	3.231526	0.003911	0.710751
-20.206111	-2.017934	3.241523	0.003808	0.710875
-20.132138	-2.031589	3.251520	0.003794	0.710874
-20.468666	-1.970972	3.261517	0.003856	0.710876
-19.540369	-2.004382	3.271514	0.003684	0.711139
-19.696726	-1.971990	3.281510	0.003713	0.711149
-19.117984	-2.077025	3.291507	0.003605	0.711145
-19.307215	-1.980397	3.301504	0.003640	0.711271
-18.614116	-2.009309	3.311501	0.003511	0.711460
-18.533404	-2.022911	3.321498	0.003496	0.711461
-18.630875	-2.004338	3.331494	0.003514	0.711464
-17.587135	-2.055450	3.341491	0.003319	0.711733
-17.687218	-2.021991	3.351488	0.003338	0.711764
-17.485405	-2.057402	3.361485	0.003300	0.711766
-17.577531	-2.019443	3.371482	0.003317	0.711809
-16.754000	-2.019998	3.381478	0.003164	0.712100
-16.513582	-2.061463	3.391475	0.003119	0.712103
-16.763999	-2.018622	3.401472	0.003165	0.712100
-16.423207	-2.011391	3.411469	0.003102	0.712235
-15.630613	-2.075808	3.421466	0.002954	0.712389
-15.772643	-2.049375	3.431462	0.002981	0.712391
-15.543492	-2.088243	3.441459	0.002938	0.712395
-15.333231	-2.004251	3.451456	0.002899	0.712637
-15.131241	-1.998334	3.461453	0.002861	0.712721
-14.776284	-2.064007	3.471450	0.002795	0.712716
-14.725734	-2.028123	3.481446	0.002785	0.712806
-13.946901	-2.047385	3.491443	0.002640	0.713044
-14.116958	-2.020945	3.501440	0.002672	0.713036
-13.867445	-2.069129	3.511437	0.002625	0.713029
-13.213861	-2.066273	3.521434	0.002503	0.713267
-13.063617	-2.042848	3.531430	0.002475	0.713367
-12.948117	-2.061504	3.541427	0.002454	0.713371
-13.129670	-2.030230	3.551424	0.002487	0.713369
-12.643077	-1.970728	3.561421	0.002397	0.713660
-12.533216	-1.988064	3.571418	0.002376	0.713664
-12.289474	-2.029641	3.581414	0.002331	0.713668
-11.640578	-2.031809	3.591411	0.002210	0.713894
-11.427343	-2.027577	3.601408	0.002170	0.713978
-11.304390	-2.048502	3.611405	0.002147	0.713980
-11.206287	-2.051829	3.621402	0.002129	0.714008
-10.347767	-2.065357	3.631398	0.001969	0.714285
-10.247312	-2.082549	3.641395	0.001950	0.714287
-10.297844	-2.073986	3.651392	0.001959	0.714286
-10.470287	-1.980890	3.661389	0.001991	0.714410
-9.568285	-2.036394	3.671386	0.001823	0.714619
-9.413950	-2.065660	3.681382	0.001794	0.714616
-9.451748	-2.058304	3.691379	0.001801	0.714618
-8.590848	-2.093382	3.701376	0.001641	0.714852
-8.412769	-2.094125	3.711373	0.001608	0.714914
-8.629606	-2.056650	3.721370	0.001648	0.714912
-8.342331	-2.106053	3.731366	0.001594	0.714916
-7.773038	-2.053375	3.741363	0.001488	0.715222
-7.516198	-2.091762	3.751360	0.001440	0.715236
-7.395054	-2.115157	3.761357	0.001418	0.715233
-7.558874	-2.057389	3.771354	0.001448	0.715290
-6.508113	-2.112288	3.781350	0.001253	0.715552
-6.549219	-2.103908	3.791347	0.001260	0.715555
-6.670224	-2.083426	3.801344	0.001282	0.715553
-6.229642	-2.080482	3.811341	0.001200	0.715714
-5.722027	-2.081296	3.821338	0.001106	0.715892
-5.573863	-2.105601	3.831334	0.001078	0.715896
-5.619729	-2.100434	3.841331	0.001087	0.715891
-5.117647	-2.112147	3.851328	0.000993	0.716045
-4.913633	-2.096747	3.861325	0.000955	0.716148
-5.073008	-2.072351	3.871322	0.000984	0.716140
-4.826633	-2.081134	3.881318	0.000939	0.716209
-3.881020	-2.125638	3.891315	0.000762	0.716455
-3.937328	-2.117075	3.901312	0.000773	0.716452
-4.063431	-2.094070	3.911309	0.000796	0.716454
-3.745154	-2.036986	3.921306	0.000737	0.716679
-2.935844	-2.136559	3.931302	0.000586	0.716767
-2.977101	-2.130441	3.941299	0.000594	0.716765
-3.018192	-2.110575	3.951296	0.000601	0.716790
-2.258854	-2.093398	3.961293	0.000460	0.717092
-2.212754	-2.102759	3.971290	0.000451	0.717090
-1.927214	-2.153576	3.981286	0.000398	0.717090
-2.057429	-2.067393	3.991283	0.000422	0.717215
-1.807400	-2.022879	4.001280	0.000375	0.717391
-1.505196	-2.078678	4.011277	0.000319	0.717388
-1.929734	-1.936221	4.021274	0.000398	0.717520
-1.408354	-1.932401	4.031270	0.000301	0.717711
-1.319503	-1.945580	4.041267	0.000284	0.717717
-1.491155	-1.786960	4.051264	0.000316	0.717970
-0.979856	-1.849821	4.061261	0.000220	0.718026
-1.020164	-1.758602	4.071258	0.000228	0.718192
-0.810774	-1.710759	4.081254	0.000189	0.718360
-0.715860	-1.685487	4.091251	0.000171	0.718444
-1.186895	-1.496582	4.101248	0.000258	0.718651
-1.023178	-1.449855	4.111245	0.000228	0.718801
-0.983288	-1.374172	4.121242	0.000220	0.718965
-0.843741	-1.270981	4.131238	0.000194	0.719218
-0.494004	-1.274154	4.141235	0.000129	0.719334
-0.531536	-1.130566	4.151232	0.000136	0.719605
-0.444853	-1.051783	4.161229	0.000119	0.719791
-0.420453	-0.974218	4.171226	0.000115	0.719952
-0.504717	-0.816004	4.181222	0.000130	0.720235
-0.489162	-0.690824	4.191219	0.000127	0.720487
-0.416573	-0.586233	4.201216	0.000114	0.720718
-0.317091	-0.487028	4.211213	0.000095	0.720949
-0.231297	-0.402507	4.221210	0.000079	0.721145
-0.304652	-0.234951	4.231206	0.000092	0.721449
-0.079101	-0.134816	4.241203	0.000050	0.721725
-0.085569	0.012883	4.251200	0.000051	0.722013
0.000000	0.161306	4.261197	0.000035	0.722335

0.259340	0.781290	4.266202	-0.000014	0.723643
0.275387	2.042692	4.271206	-0.000018	0.726117
0.311987	3.894537	4.276211	-0.000026	0.729740
0.733827	6.231743	4.281216	-0.000106	0.734415
0.899580	9.116749	4.286221	-0.000139	0.740024
1.260631	12.457860	4.291226	-0.000208	0.746525
1.647979	16.243286	4.296230	-0.000283	0.753815
2.111672	20.420633	4.301235	-0.000372	0.761790
2.426264	25.029247	4.306240	-0.000433	0.770428
2.749797	29.994335	4.311245	-0.000497	0.779623
3.746774	35.197834	4.316250	-0.000686	0.789353
4.082974	40.836569	4.321254	-0.000752	0.799529
4.473600	46.769171	4.326259	-0.000829	0.810109
4.933081	52.970713	4.331264	-0.000919	0.821038
5.327242	59.455874	4.336269	-0.000996	0.832288
6.029915	66.109388	4.341274	-0.001131	0.843761
6.598455	73.011951	4.346278	-0.001242	0.855454
10.540093	79.546808	4.351283	-0.001980	0.867359
11.284983	86.886494	4.356288	-0.002124	0.879492
11.581123	94.456278	4.361293	-0.002184	0.891700
12.465750	102.088460	4.366298	-0.002354	0.904003
13.378422	109.860096	4.371302	-0.002529	0.916364
14.054977	117.787294	4.376307	-0.002660	0.928734
15.036983	125.796727	4.381312	-0.002848	0.941146
15.540055	133.976074	4.386317	-0.002947	0.953523
16.637999	142.144274	4.391322	-0.003157	0.965878
17.730754	150.398153	4.396326	-0.003366	0.978199
18.606856	158.775393	4.401331	-0.003534	0.990489
19.739356	167.142742	4.406336	-0.003751	1.002676
20.364409	175.645416	4.411341	-0.003873	1.014783
21.133909	184.163194	4.416346	-0.004021	1.026802
22.278855	192.656264	4.421350	-0.004240	1.038736
23.380849	201.193458	4.426355	-0.004451	1.050584
24.381393	209.780351	4.431360	-0.004643	1.062342
25.100854	218.433886	4.436365	-0.004783	1.073994
25.882925	227.073512	4.441370	-0.004934	1.085517
26.568741	235.746531	4.446374	-0.005067	1.096940
27.063730	244.448432	4.451379	-0.005165	1.108240
27.937959	253.096904	4.456384	-0.005334	1.119441
28.606777	261.750797	4.461389	-0.005464	1.130492
29.515360	270.388597	4.466394	-0.005639	1.141468
30.016721	279.108108	4.471398	-0.005738	1.152353
30.827458	287.725930	4.476403	-0.005894	1.163076
31.496078	296.362503	4.481408	-0.006025	1.173695
32.212277	304.961978	4.486413	-0.006164	1.184183
32.908464	313.580747	4.491418	-0.006299	1.194597
33.181253	322.229788	4.496422	-0.006355	1.204872
34.107133	330.771190	4.501427	-0.006533	1.215064
34.959140	339.315762	4.506432	-0.006698	1.225160
35.571532	347.906487	4.511437	-0.006817	1.235179
36.620879	356.388713	4.516442	-0.007018	1.245078
36.921834	364.990235	4.521446	-0.007080	1.254890
37.223051	373.565210	4.526451	-0.007142	1.264597
38.119582	382.031914	4.531456	-0.007314	1.274220
38.871448	390.492488	4.536461	-0.007460	1.283737
39.485339	399.000401	4.541466	-0.007580	1.293210
40.100718	407.468357	4.546470	-0.007700	1.302571
40.793877	416.002766	4.551475	-0.007834	1.311951
41.591353	424.473879	4.556480	-0.007988	1.321214
42.160694	432.893504	4.561485	-0.008100	1.330317
42.824218	441.302185	4.566490	-0.008229	1.339363
43.348863	449.721234	4.571494	-0.008332	1.348335
43.704438	458.159939	4.576499	-0.008404	1.357238
44.684345	466.464861	4.581504	-0.008592	1.366052
45.213271	474.862458	4.586509	-0.008696	1.374827
45.846508	483.227195	4.591514	-0.008819	1.383531
46.419846	491.614650	4.596518	-0.008932	1.392193
47.043318	499.954409	4.601523	-0.009053	1.400761
47.301434	508.356712	4.606528	-0.009107	1.409279
47.772648	516.711395	4.611533	-0.009200	1.417733
48.354993	525.030823	4.616538	-0.009314	1.426120
49.281847	533.310162	4.621542	-0.009492	1.434475
49.817385	541.622363	4.626547	-0.009597	1.442749
50.313822	549.951500	4.631552	-0.009695	1.450987
50.911940	558.244363	4.636557	-0.009812	1.459158
51.390951	566.569232	4.641562	-0.009907	1.467296
51.714209	574.956812	4.646566	-0.009972	1.475425
52.386136	583.187353	4.651571	-0.010103	1.483413
52.971087	591.464123	4.656576	-0.010217	1.491389
53.338952	599.760687	4.661581	-0.010291	1.499307
53.969302	608.011049	4.666586	-0.010414	1.507181
54.461027	616.288610	4.671590	-0.010511	1.515017
55.011688	624.541085	4.676595	-0.010619	1.522799
55.696092	632.783109	4.681600	-0.010752	1.530551
56.672135	640.966127	4.686605	-0.010939	1.538253
57.032454	649.257454	4.691610	-0.011011	1.545924
57.304838	657.563623	4.696614	-0.011067	1.553558
57.767297	665.792259	4.701619	-0.011159	1.561112
58.436740	674.007567	4.706624	-0.011289	1.568647
58.710884	682.273992	4.711629	-0.011346	1.576135
59.157167	690.506859	4.716634	-0.011434	1.583582
59.922597	698.694088	4.721638	-0.011582	1.590999
60.355182	706.932711	4.726643	-0.011668	1.598380
60.840908	715.151022	4.731648	-0.011764	1.605716
61.241939	723.385194	4.736653	-0.011844	1.613021
61.786510	731.588531	4.741658	-0.011951	1.620285
62.194283	739.811578	4.746662	-0.012032	1.627515
62.670117	748.072732	4.751667	-0.012126	1.634756
63.397484	756.213577	4.756672	-0.012267	1.641895
63.729629	764.423453	4.761677	-0.012334	1.649008
64.094168	772.635391	4.766682	-0.012407	1.656097
64.943635	780.760143	4.771686	-0.012571	1.663146
65.327557	788.965630	4.776691	-0.012648	1.670172
65.734721	797.186922	4.781696	-0.012729	1.677184
65.987057	805.384629	4.786701	-0.012781	1.684127
66.281358	813.609662	4.791706	-0.012841	1.691069
66.735641	821.789156	4.796710	-0.012931	1.697966
67.127616	829.958133	4.801715	-0.013010	1.704818
67.629573	838.149155	4.806720	-0.013109	1.711675
68.160433	846.306732	4.811725	-0.013213	1.718481
68.649991	854.456751	4.816730	-0.013309	1.725248
69.237658	862.604077	4.821734	-0.013424	1.731999
69.744863	870.766339	4.826739	-0.013524	1.738725
70.195678	878.920907	4.831744	-0.013613	1.745412
70.480050	887.117785	4.836749	-0.013672	1.752086
71.141743	895.253078	4.841754	-0.013800	1.758733
71.684064	903.379091	4.846758	-0.013906	1.765332
72.043640	911.571739	4.851763	-0.013979	1.771937
72.684773	919.711021	4.856768	-0.014103	1.778510
73.075668	927.868747	4.861773	-0.014182	1.785042
73.556989	936.070404	4.866778	-0.014277	1.791595
73.894902	944.256610	4.871782	-0.014345	1.798096
74.153293	952.410297	4.876787	-0.014398	1.804537
74.606319	960.542991	4.881792	-0.014488	1.810963
74.945977	968.676034	4.886797	-0.014557	1.817352
75.593098	976.775633	4.891802	-0.014683	1.823730
76.046309	984.917300	4.896806	-0.014772	1.830094
76.236056	993.096442	4.901811	-0.014813	1.836434
76.669384	1001.224651	4.906816	-0.014899	1.842742
77.129246	1009.357714	4.911821	-0.014990	1.849035
77.449511	1017.515138	4.916826	-0.015055	1.855309
78.176154	1025.593059	4.921830	-0.015196	1.861548
78.477523	1033.752337	4.926835	-0.015257	1.867779
78.828894	1041.952205	4.931840	-0.015328	1.874026
78.978895	1050.083564	4.936845	-0.015361	1.880176
79.436521	1058.195170	4.941850	-0.015452	1.886327
79.996078	1066.306745	4.946854	-0.015561	1.892470
80.285219	1074.443699	4.951859	-0.015620	1.898580
80.587059	1082.580660	4.956864	-0.015682	1.904673
80.951949	1090.709157	4.961869	-0.015755	1.910747
81.454801	1098.822115	4.966874	-0.015854	1.916805
81.783485	1106.939343	4.971878	-0.015921	1.922828
82.214535	1115.039061	4.976883	-0.016006	1.928830
82.819594	1123.146349	4.981888	-0.016124	1.934838
83.090380	1131.270955	4.986893	-0.016180	1.940804
83.883207	1139.346812	4.991898	-0.016333	1.946772
84.131702	1147.545196	4.996902	-0.016385	1.952752
84.599193	1155.652610	5.001907	-0.016477	1.958672
85.026022	1163.751405	5.006912	-0.016562	1.964563
85.469276	1171.835507	5.011917	-0.016650	1.970427
85.922316	1179.943504	5.016922	-0.016739	1.976292
86.279014	1188.066064	5.021926	-0.016811	1.982140
86.670617	1196.167192	5.026931	-0.016889	1.987959
86.940454	1204.345871	5.031936	-0.016945	1.993802
87.460076	1212.398221	5.036941	-0.017047	1.999566
87.758718	1220.503861	5.041946	-0.017108	2.005327
88.144352	1228.620667	5.046950	-0.017185	2.011089
88.551221	1236.720368	5.051955	-0.017266	2.016824
89.138814	1244.787846	5.056960	-0.017381	2.022539
89.489284	1252.893192	5.061965	-0.017451	2.028240
89.894090	1261.054709	5.066970	-0.017532	2.033969
90.132757	1269.153084	5.071974	-0.017582	2.039622
90.514667	1277.231710	5.076979	-0.017658	2.045259
91.024625	1285.324157	5.081984	-0.017759	2.050904
91.331910	1293.441742	5.086989	-0.017821	2.056529
91.829944	1301.524177	5.091994	-0.017919	2.062135
92.163699	1309.639062	5.096998	-0.017987	2.067730
92.249731	1317.791018	5.102003	-0.018008	2.073312
92.603337	1325.902275	5.107008	-0.018079	2.078877
93.006754	1333.947869	5.112013	-0.018160	2.084387
93.334763	1342.052069	5.117018	-0.018226	2.089915
93.804073	1350.156152	5.122022	-0.018319	2.095442
94.373751	1358.188717	5.127027	-0.018430	2.100916
94.924746	1366.283723	5.132032	-0.018538	2.106416
95.162855	1374.423792	5.137037	-0.018588	2.111901
95.918974	1382.501047	5.142042	-0.018734	2.117380
96.346839	1390.552440	5.147046	-0.018819	2.122795
96.564609	1398.659372	5.152051	-0.018865	2.128214
96.841666	1406.790648	5.157056	-0.018922	2.133641
97.192886	1414.852013	5.162061	-0.018992	2.139014
97.662472	1422.925990	5.167066	-0.019085	2.144394
97.865778	1431.041336	5.172070	-0.019128	2.149762
98.471801	1439.103294	5.177075	-0.019246	2.155119
98.967267	1447.176509	5.182080	-0.019344	2.160460
98.862810	1455.298561	5.187085	-0.019330	2.165764
99.170343	1463.407089	5.192090	-0.019392	2.171084
99.745955	1471.476842	5.197094	-0.019505	2.176391
99.959973	1479.559228	5.202099	-0.019550	2.181659
100.616614	1487.607405	5.207104	-0.019678	2.186934
100.857633	1495.739294	5.212109	-0.019728	2.192211
100.911427	1503.859442	5.217114	-0.019743	2.197451
101.339723	1511.904001	5.222118	-0.019828	2.202664
101.740902	1519.961772	5.227123	-0.019908	2.207871
102.186511	1528.041175	5.232128	-0.019996	2.213083
102.283817	1536.143787	5.237133	-0.020020	2.218266
102.681322	1544.210882	5.242138	-0.020099	2.223441
103.230067	1552.267808	5.247142	-0.020207	2.228612
103.508172	1560.374753	5.252147	-0.020264	2.233777
103.729237	1568.468372	5.257152	-0.020310	2.238918
104.075765	1576.515758	5.262157	-0.020380	2.244028
104.485489	1584.598519	5.267162	-0.020462	2.249155
104.559010	1592.734033	5.272166	-0.020481	2.254273
104.702757	1600.794113	5.277171	-0.020513	2.259339
105.304619	1608.845185	5.282176	-0.020630	2.264427
105.487520	1616.929672	5.287181	-0.020670	2.269489
105.881164	1625.091336	5.292186	-0.020748	2.274605
106.338403	1633.103690	5.297190	-0.020839	2.279623
106.735142	1641.127992	5.302195	-0.020918	2.284631
107.298488	1649.182401	5.307200	-0.021028	2.289662
107.597188	1657.269742	5.312205	-0.021089	2.294679
108.234042	1665.291855	5.317210	-0.021213	2.299673
108.465511	1673.375149	5.322214	-0.021261	2.304660
108.663572	1681.460050	5.327219	-0.021303	2.309634
109.154525	1689.561371	5.332224	-0.021400	2.314632
109.193021	1697.638055	5.337229	-0.021413	2.319567
109.609713	1705.678195	5.342234	-0.021495	2.324500
110.029967	1713.741141	5.347238	-0.021579	2.329437
110.239483	1721.856013	5.352243	-0.021623	2.334377
110.582557	1729.913346	5.357248	-0.021692	2.339283
111.153472	1737.919762	5.362253	-0.021804	2.344166
111.817581	1745.982264	5.367258	-0.021933	2.349081
111.990099	1754.130774	5.372262	-0.021970	2.353997
112.157357	1762.198761	5.377267	-0.022007	2.358854
112.617902	1770.247441	5.382272	-0.022098	2.363712
112.991813	1778.279684	5.387277	-0.022173	2.368545
113.200355	1786.392414	5.392282	-0.022217	2.373401
113.428734	1794.458371	5.397286	-0.022265	2.378222
113.927095	1802.481086	5.402291	-0.022363	2.383029
114.341443	1810.554749	5.407296	-0.022445	2.387849
114.716297	1818.613313	5.412301	-0.022520	2.392648
114.996981	1826.713288	5.417306	-0.022578	2.397454
115.368927	1834.764295	5.422310	-0.022653	2.402228
115.646429	1842.807720	5.427315	-0.022710	2.406981
115.901540	1850.908532	5.432320	-0.022762	2.411757
116.170066	1858.979002	5.437325	-0.022818	2.416506
116.594997	1867.030438	5.442330	-0.022902	2.421247
116.755892	1875.107079	5.447334	-0.022937	2.425973
117.147573	1883.197348	5.452339	-0.023016	2.430715
117.366272	1891.342030	5.457344	-0.023062	2.435467
117.674458	1899.350165	5.462349	-0.023124	2.440136
118.314433	1907.335732	5.467354	-0.023249	2.444809
118.777861	1915.383640	5.472358	-0.023340	2.449496
119.126277	1923.439829	5.477363	-0.023411	2.454169
119.383945	1931.521015	5.482368	-0.023464	2.458841
119.697778	1939.554958	5.487373	-0.023528	2.463481
119.963382	1947.629607	5.492378	-0.023582	2.468133
120.178353	1955.720245	5.497382	-0.023628	2.472780
120.394442	1963.768685	5.502387	-0.023673	2.477395
120.559773	1971.839131	5.507392	-0.023709	2.482010
120.845535	1979.865217	5.512397	-0.023768	2.486600
121.289360	1987.930178	5.517402	-0.023856	2.491216
121.487491	1996.023344	5.522406	-0.023898	2.495820
121.417427	2004.090786	5.527411	-0.023890	2.500382
121.755698	2012.137286	5.532416	-0.023958	2.504954
122.157568	2020.157026	5.537421	-0.024038	2.509507
122.721392	2028.245203	5.542426	-0.024149	2.514101
122.840782	2036.320075	5.547430	-0.024176	2.518648
123.043720	2044.345749	5.552435	-0.024219	2.523164
123.525095	2052.378591	5.557440	-0.024314	2.527697
124.017452	2060.425042	5.562445	-0.024411	2.532230
124.125168	2068.522836	5.567450	-0.024437	2.536755
124.595496	2076.538338	5.572454	-0.024529	2.541253
124.753652	2084.589100	5.577459	-0.024564	2.545740
125.055396	2092.690045	5.582464	-0.024626	2.550257
125.297928	2100.743094	5.587469	-0.024676	2.554736
125.819448	2108.747249	5.592474	-0.024779	2.559198
125.998722	2116.815913	5.597478	-0.024817	2.563665
126.298221	2124.858409	5.602483	-0.024878	2.568118
126.629969	2132.938554	5.607488	-0.024945	2.572586
126.752624	2140.993753	5.612493	-0.024974	2.577018
127.293919	2149.025294	5.617498	-0.025080	2.581459
127.623246	2157.078667	5.622502	-0.025146	2.585889
127.767620	2165.178586	5.627507	-0.025178	2.590324
128.264553	2173.395786	5.632512	-0.025276	2.594839
128.822418	2181.333930	5.637517	-0.025385	2.599199
129.218154	2189.343546	5.642522	-0.025464	2.603579
129.660823	2197.368273	5.647526	-0.025552	2.607963
130.074697	2205.386408	5.652531	-0.025634	2.612334
130.322230	2213.477801	5.657536	-0.025686	2.616726
130.315122	2221.529884	5.662541	-0.025690	2.621073
130.635400	2229.563970	5.667546	-0.025755	2.625424
130.939318	2237.608662	5.672550	-0.025817	2.629773
131.139735	2245.684814	5.677555	-0.025859	2.634125
131.634533	2253.707460	5.682560	-0.025957	2.638460
131.823683	2261.746605	5.687565	-0.025997	2.642776
132.000535	2269.792628	5.692570	-0.026035	2.647089
132.312555	2277.861731	5.697574	-0.026099	2.651415
132.597517	2285.899418	5.702579	-0.026157	2.655716
132.818929	2293.965093	5.707584	-0.026204	2.660021
133.000482	2301.992922	5.712589	-0.026243	2.664296
133.014066	2310.072401	5.717594	-0.026251	2.668580
133.653526	2318.111523	5.722598	-0.026375	2.672877
133.761692	2326.182083	5.727603	-0.026400	2.677149
134.195195	2334.198507	5.732608	-0.026486	2.681407
134.353516	2342.235592	5.737613	-0.026521	2.685651
134.675073	2350.274763	5.742618	-0.026586	2.689899
134.968647	2358.344482	5.747622	-0.026646	2.694156
135.333967	2366.361331	5.752627	-0.026719	2.698382
135.827135	2374.392973	5.757632	-0.026817	2.702617
135.875602	2382.484083	5.762637	-0.026831	2.706849
136.115700	2390.544071	5.767642	-0.026881	2.711070
136.409775	2398.609139	5.772646	-0.026941	2.715290
136.428624	2406.621766	5.777651	-0.026950	2.719460
136.689632	2414.673298	5.782656	-0.027004	2.723658
136.895591	2422.692727	5.787661	-0.027047	2.727830
137.297334	2430.737595	5.792666	-0.027127	2.732020
137.537659	2438.841318	5.797670	-0.027177	2.736224
137.870947	2446.818375	5.802675	-0.027245	2.740362
138.051882	2454.872909	5.807680	-0.027284	2.744525
138.194124	2462.941902	5.812685	-0.027316	2.748686
138.741118	2471.018278	5.817690	-0.027423	2.752870
139.067800	2479.086182	5.822694	-0.027489	2.757029
139.078916	2487.111281	5.827699	-0.027496	2.761141
139.252273	2495.145295	5.832704	-0.027534	2.765261
139.546688	2503.165665	5.837709	-0.027594	2.769375
140.110987	2511.196749	5.842714	-0.027704	2.773504
140.476056	2519.247938	5.847718	-0.027777	2.777626
140.669770	2527.259284	5.852723	-0.027819	2.781711
141.321981	2535.274362	5.857728	-0.027945	2.785819
141.371928	2543.354000	5.862733	-0.027960	2.789918
141.460503	2551.452827	5.867738	-0.027982	2.794023
142.115432	2559.462542	5.872742	-0.028109	2.798110
142.336681	2567.477264	5.877747	-0.028156	2.802169
142.660062	2575.537885	5.882752	-0.028221	2.806250
142.910812	2583.570953	5.887757	-0.028273	2.810308
143.359438	2591.622984	5.892762	-0.028362	2.814380
143.518530	2599.694474	5.897766	-0.028397	2.818439
143.864357	2607.685334	5.902771	-0.028466	2.822463
144.255612	2615.740070	5.907776	-0.028545	2.826516
144.512914	2623.791172	5.912781	-0.028598	2.830553
144.762112	2631.878635	5.917786	-0.028649	2.834603
145.058457	2639.886562	5.922790	-0.028710	2.838609
145.172030	2647.920350	5.927795	-0.028736	2.842612
145.490556	2655.971968	5.932800	-0.028801	2.846630
145.828552	2663.977537	5.937805	-0.028869	2.850621
145.898825	2672.084525	5.942810	-0.028888	2.854641
146.227076	2680.100781	5.947814	-0.028954	2.858625
146.564043	2688.100871	5.952819	-0.029022	2.862596
147.051921	2696.128316	5.957824	-0.029118	2.866583
147.363387	2704.176127	5.962829	-0.029181	2.870565
147.607701	2712.244044	5.967834	-0.029232	2.874547
148.052212	2720.270497	5.972838	-0.029320	2.878515
148.176893	2728.296665	5.977843	-0.029349	2.882459
148.189220	2736.380154	5.982848	-0.029356	2.886420
148.668331	2744.382243	5.987853	-0.029451	2.890361
149.072157	2752.456912	5.992858	-0.029531	2.894328
149.182877	2760.520136	5.997862	-0.029557	2.898268
149.371331	2768.522365	6.002867	-0.029598	2.902177
149.884384	2776.557618	6.007872	-0.029698	2.906114
149.981003	2784.611146	6.012877	-0.029722	2.910032
150.532492	2792.709493	6.017882	-0.029830	2.913991
150.866115	2800.703068	6.022886	-0.029897	2.917883
151.090260	2808.736226	6.027891	-0.029944	2.921782
151.436323	2816.753396	6.032896	-0.030014	2.925675
151.559330	2824.779140	6.037901	-0.030042	2.929555
151.777334	2832.860385	6.042906	-0.030088	2.933461
151.995124	2840.901928	6.047910	-0.030134	2.937344
152.244130	2848.913168	6.052915	-0.030185	2.941208
152.786056	2856.906733	6.057920	-0.030291	2.945073
153.024101	2864.958160	6.062925	-0.030341	2.948946
153.052254	2873.036997	6.067930	-0.030352	2.952816
153.729357	2881.069889	6.072934	-0.030483	2.956692
153.883957	2889.077414	6.077939	-0.030517	2.960524
154.088983	2897.139140	6.082944	-0.030560	2.964379
154.116641	2905.175966	6.087949	-0.030571	2.968208
154.650420	2913.191614	6.092954	-0.030676	2.972048
154.743474	2921.298313	6.097958	-0.030698	2.975904
154.837539	2929.299592	6.102963	-0.030721	2.979706
155.151928	2937.328023	6.107968	-0.030785	2.983526
155.324805	2945.360755	6.112973	-0.030822	2.987336
155.550401	2953.417446	6.117978	-0.030870	2.991155
156.097718	2961.461263	6.122982	-0.030977	2.994979
156.570666	2969.428051	6.127987	-0.031070	2.998758
157.009597	2977.457816	6.132992	-0.031157	3.002560
157.333838	2985.486093	6.137997	-0.031223	3.006351
157.667158	2993.513755	6.143002	-0.031290	3.010138
157.994031	3001.594341	6.148006	-0.031356	3.013944
158.072038	3009.662557	6.153011	-0.031376	3.017727
158.192491	3017.710493	6.158016	-0.031404	3.021498
158.548822	3025.701960	6.163021	-0.031475	3.025250
158.797290	3033.750857	6.168026	-0.031527	3.029018
159.067853	3041.815675	6.173030	-0.031583	3.032790
159.166664	3049.868135	6.178035	-0.031606	3.036543
159.297169	3057.873602	6.183040	-0.031636	3.040271
159.522669	3065.886608	6.188045	-0.031683	3.044003
159.849187	3073.915374	6.193050	-0.031749	3.047742
160.154187	3081.976613	6.198054	-0.031811	3.051491
160.297505	3090.015159	6.203059	-0.031843	3.055217
160.635136	3098.042431	6.208064	-0.031911	3.058942
161.191624	3106.048594	6.213069	-0.032020	3.062663
161.316486	3114.109317	6.218074	-0.032049	3.066384
161.854435	3122.123770	6.223078	-0.032154	3.070099
162.290620	3130.212185	6.228083	-0.032241	3.073839
162.500735	3138.253252	6.233088	-0.032285	3.077542
162.498052	3146.279940	6.238093	-0.032290	3.081223
162.836881	3154.268240	6.243098	-0.032358	3.084899
163.081127	3162.318070	6.248102	-0.032409	3.088594
163.292152	3170.361181	6.253107	-0.032454	3.092280
163.637267	3178.406067	6.258112	-0.032523	3.095968
163.806570	3186.411824	6.263117	-0.032560	3.099626
163.881241	3194.456452	6.268122	-0.032579	3.103293
164.105399	3202.504705	6.273126	-0.032626	3.106964
164.254644	3210.530155	6.278131	-0.032659	3.110617
164.951847	3218.557667	6.283136	-0.032794	3.114292
165.222642	3226.559978	6.288141	-0.032850	3.117931
165.458420	3234.596627	6.293146	-0.032899	3.121580
165.809588	3242.630067	6.298150	-0.032970	3.125228
165.883510	3250.663661	6.303155	-0.032989	3.128860
166.194622	3258.722848	6.308160	-0.033052	3.132510
166.559411	3266.775254	6.313165	-0.033125	3.136154
166.998485	3274.749458	6.318170	-0.033212	3.139763
167.102873	3282.828912	6.323174	-0.033237	3.143400
167.275619	3290.842960	6.328179	-0.033275	3.147006
167.653358	3298.870775	6.333184	-0.033350	3.150623
167.870581	3306.950755	6.338189	-0.033396	3.154252
168.034648	3314.970603	6.343194	-0.033432	3.157848
168.333921	3323.013895	6.348198	-0.033493	3.161456
168.222321	3330.994844	6.353203	-0.033477	3.165015
168.663376	3339.024086	6.358208	-0.033565	3.168614
169.234504	3347.038997	6.363213	-0.033676	3.172209
169.230703	3355.089521	6.368218	-0.033681	3.175791
169.490662	3363.111301	6.373222	-0.033735	3.179367
169.776584	3371.129223	6.378227	-0.033793	3.182939
170.224808	3379.161295	6.383232	-0.033882	3.186519
170.348638	3387.210144	6.388237	-0.033910	3.190090
170.550514	3395.284695	6.393242	-0.033953	3.193671
170.940276	3403.301889	6.398246	-0.034031	3.197230
171.092249	3411.315263	6.403251	-0.034064	3.200774
171.290187	3419.347442	6.408256	-0.034107	3.204324
171.513268	3427.377764	6.413261	-0.034153	3.207870
171.660295	3435.427057	6.418266	-0.034186	3.211418
171.978041	3443.465811	6.423270	-0.034250	3.214964
172.271695	3451.475295	6.428275	-0.034310	3.218492
172.776738	3459.486145	6.433280	-0.034410	3.222025
172.953468	3467.510883	6.438285	-0.034448	3.225548
173.272640	3475.546271	6.443290	-0.034513	3.229076
173.624155	3483.652660	6.448294	-0.034583	3.232634
173.878902	3491.704114	6.453299	-0.034636	3.236159
174.144604	3499.686830	6.458304	-0.034691	3.239651
174.387204	3507.686874	6.463309	-0.034741	3.243146
174.396857	3515.718482	6.468314	-0.034748	3.246641
174.515877	3523.741558	6.473318	-0.034776	3.250133
174.774533	3531.776399	6.478323	-0.034829	3.253633
175.231277	3539.810609	6.483328	-0.034920	3.257135
175.303822	3547.837460	6.488333	-0.034938	3.260616
175.520638	3555.831689	6.493338	-0.034984	3.264085
176.013712	3563.878873	6.498342	-0.035081	3.267583
176.063850	3571.919268	6.503347	-0.035096	3.271058
176.178743	3579.991366	6.508352	-0.035122	3.274545
176.448517	3588.004560	6.513357	-0.035178	3.278009
176.684001	3596.020740	6.518362	-0.035227	3.281469
176.756708	3604.031032	6.523366	-0.035246	3.284916
176.955216	3612.057440	6.528371	-0.035288	3.288372
177.592614	3620.109298	6.533376	-0.035412	3.291852
177.697950	3628.161239	6.538381	-0.035437	3.295308
177.745309	3636.168484	6.543386	-0.035451	3.298738
178.065588	3644.190582	6.548390	-0.035516	3.302182
178.285787	3652.191324	6.553395	-0.035562	3.305610
178.545540	3660.260654	6.558400	-0.035616	3.309064
178.964845	3668.284220	6.563405	-0.035699	3.312501
179.418164	3676.316278	6.568410	-0.035789	3.315940
179.546534	3684.344266	6.573414	-0.035818	3.319361
179.633790	3692.340847	6.578419	-0.035840	3.322764
180.072603	3700.385622	6.583424	-0.035927	3.326196
180.090027	3708.404914	6.588429	-0.035935	3.329599
180.466165	3716.441078	6.593434	-0.036010	3.333019
180.686257	3724.502155	6.598438	-0.036057	3.336439
180.926181	3732.447299	6.603443	-0.036107	3.339808
181.373715	3740.478056	6.608448	-0.036195	3.343217
181.458782	3748.531400	6.613453	-0.036216	3.346620
181.811575	3756.541850	6.618458	-0.036287	3.350010
182.033420	3764.625945	6.623462	-0.036334	3.353423
182.204379	3772.667803	6.628467	-0.036371	3.356813
182.641138	3780.655833	6.633472	-0.036458	3.360186
182.695974	3788.708397	6.638477	-0.036473	3.363569
182.874968	3796.745162	6.643482	-0.036512	3.366947
183.167046	3804.770826	6.648486	-0.036571	3.370321
183.251370	3812.808051	6.653491	-0.036592	3.373688
183.465729	3820.875258	6.658496	-0.036638	3.377070
183.875491	3828.844518	6.663501	-0.036719	3.380414
184.065751	3836.873210	6.668506	-0.036760	3.383771
184.344455	3844.910064	6.673510	-0.036817	3.387132
184.540833	3852.923671	6.678515	-0.036859	3.390477
184.991312	3861.041224	6.683520	-0.036948	3.393871
185.134059	3869.029649	6.688525	-0.036980	3.397197
185.233869	3877.009981	6.693530	-0.037004	3.400514
185.662655	3885.026665	6.698534	-0.037089	3.403855
185.811614	3893.025538	6.703539	-0.037122	3.407176
185.965279	3901.079428	6.708544	-0.037156	3.410516
186.001816	3909.109382	6.713549	-0.037168	3.413839
186.308649	3917.137136	6.718554	-0.037230	3.417167
186.655270	3925.163566	6.723558	-0.037300	3.420493
186.676800	3933.166168	6.728563	-0.037309	3.423794
186.933675	3941.211950	6.733568	-0.037362	3.427118
187.311387	3949.243728	6.738573	-0.037438	3.430437
187.364578	3957.264924	6.743578	-0.037453	3.433738
187.638042	3965.339186	6.748582	-0.037509	3.437064
187.971711	3973.304694	6.753587	-0.037577	3.440345
188.223516	3981.347006	6.758592	-0.037629	3.443651
188.381755	3989.374173	6.763597	-0.037664	3.446945
188.892721	3997.377084	6.768602	-0.037764	3.450237
189.029498	4005.446757	6.773606	-0.037795	3.453541
189.123592	4013.477159	6.778611	-0.037818	3.456824
189.340334	4021.510871	6.783616	-0.037863	3.460110
189.800462	4029.513908	6.788621	-0.037954	3.463388
190.139929	4037.551916	6.793626	-0.038023	3.466673
190.390513	4045.613926	6.798630	-0.038075	3.469961
190.588197	4053.650986	6.803635	-0.038117	3.473235
190.842342	4061.709762	6.808640	-0.038169	3.476516
190.841052	4069.645373	6.813645	-0.038174	3.479736
191.005210	4077.661731	6.818650	-0.038210	3.482991
191.321535	4085.698514	6.823654	-0.038274	3.486256
191.416632	4093.692993	6.828659	-0.038297	3.489494
191.769830	4101.759965	6.833664	-0.038368	3.492766
191.968111	4109.780122	6.838669	-0.038411	3.496012
192.042201	4117.795718	6.843674	-0.038430	3.499248
192.347110	4125.819646	6.848678	-0.038492	3.502492
192.601542	4133.803842	6.853683	-0.038544	3.505716
192.865572	4141.863866	6.858688	-0.038599	3.508967
193.117542	4149.888903	6.863693	-0.038651	3.512201
193.555597	4157.903427	6.868698	-0.038738	3.515433
193.834735	4165.936028	6.873702	-0.038795	3.518665
193.852210	4173.978018	6.878707	-0.038804	3.521889
194.160881	4181.971115	6.883712	-0.038866	3.525100
194.470957	4190.004328	6.888717	-0.038929	3.528324
194.524297	4198.050238	6.893722	-0.038945	3.531542
194.459889	4206.170982	6.898726	-0.038938	3.534783
194.671782	4214.149385	6.903731	-0.038983	3.537973
194.945334	4222.161057	6.908736	-0.039039	3.541176
195.065753	4230.155413	6.913741	-0.039066	3.544363
195.292196	4238.157026	6.918746	-0.039114	3.547554
195.734654	4246.212061	6.923750	-0.039202	3.550770
195.940145	4254.354182	6.928755	-0.039245	3.554010
196.178304	4262.373153	6.933760	-0.039295	3.557200
196.395324	4270.327728	6.938765	-0.039340	3.560360
196.712712	4278.285297	6.943770	-0.039405	3.563522
197.056681	4286.350735	6.948774	-0.039474	3.566724
197.356035	4294.314671	6.953779	-0.039535	3.569882
197.703698	4302.391398	6.958784	-0.039605	3.573083
198.003894	4310.418037	6.963789	-0.039666	3.576260
198.265924	4318.409567	6.968794	-0.039720	3.579419
198.699214	4326.426888	6.973798	-0.039806	3.582590
198.606325	4334.451155	6.978803	-0.039794	3.585747
198.923510	4342.507932	6.983808	-0.039859	3.588925
199.162168	4350.537862	6.988813	-0.039908	3.592087
199.425470	4358.543798	6.993818	-0.039963	3.595238
199.900646	4366.540270	6.998822	-0.040056	3.598388
200.093034	4374.582296	7.003827	-0.040097	3.601545
200.384410	4382.550315	7.008832	-0.040157	3.604673
200.468808	4390.641334	7.013837	-0.040178	3.607841
200.609080	4398.640510	7.018842	-0.040209	3.610972
201.004865	4406.696010	7.023846	-0.040288	3.614129
201.142087	4414.702329	7.028851	-0.040319	3.617257
201.352273	4422.737812	7.033856	-0.040364	3.620395
201.472298	4430.758557	7.038861	-0.040391	3.623523
201.767224	4438.775006	7.043866	-0.040451	3.626651
201.918503	4446.833318	7.048870	-0.040485	3.629789
201.978442	4454.872800	7.053875	-0.040501	3.632914
202.286670	4462.924750	7.058880	-0.040564	3.636048
202.241215	4470.922605	7.063885	-0.040561	3.639148
202.397810	4478.932841	7.068890	-0.040595	3.642257
202.750432	4486.917317	7.073894	-0.040666	3.645357
203.157885	4494.939759	7.078899	-0.040747	3.648472
203.242133	4502.995123	7.083904	-0.040768	3.651587
203.526789	4511.022884	7.088909	-0.040826	3.654695
203.698629	4519.026337	7.093914	-0.040864	3.657788
204.071371	4527.070992	7.098918	-0.040938	3.660899
204.105774	4535.063363	7.103923	-0.040950	3.663978
204.563892	4543.101627	7.108928	-0.041041	3.667084
204.739159	4551.125084	7.113933	-0.041079	3.670174
204.993171	4559.177002	7.118938	-0.041131	3.673274
205.441433	4567.209196	7.123942	-0.041220	3.676369
205.467356	4575.195536	7.128947	-0.041230	3.679433
205.432060	4583.221091	7.133952	-0.041229	3.682507
205.826243	4591.187740	7.138957	-0.041307	3.685568
205.986028	4599.240966	7.143962	-0.041342	3.688653
206.110262	4607.316397	7.148966	-0.041371	3.691743
206.199811	4615.324041	7.153971	-0.041393	3.694804
206.678248	4623.339434	7.158976	-0.041487	3.697875
206.815222	4631.364048	7.163981	-0.041518	3.700938
206.901523	4639.364203	7.168986	-0.041539	3.703988
207.150615	4647.429493	7.173990	-0.041591	3.707065
207.651843	4655.392723	7.178995	-0.041689	3.710106
207.822910	4663.504529	7.184000	-0.041727	3.713193
207.931070	4671.565472	7.189005	-0.041752	3.716257
208.276631	4679.490520	7.194010	-0.041822	3.719272
208.449559	4687.531078	7.199014	-0.041859	3.722324
208.507981	4695.494818	7.204019	-0.041875	3.725342
208.879641	4703.522995	7.209024	-0.041950	3.728390
209.293583	4711.555273	7.214029	-0.042032	3.731437
209.137498	4719.607475	7.219034	-0.042008	3.734476
209.511443	4727.634111	7.224038	-0.042083	3.737515
209.656097	4735.635274	7.229043	-0.042115	3.740537
209.666326	4743.655410	7.234048	-0.042123	3.743560
209.853200	4751.693573	7.239053	-0.042163	3.746592
210.139118	4759.686623	7.244058	-0.042221	3.749607
210.829446	4767.762047	7.249062	-0.042355	3.752659
210.659444	4775.782011	7.254067	-0.042329	3.755668
211.033204	4783.782834	7.259072	-0.042403	3.758681
211.273736	4791.842434	7.264077	-0.042454	3.761709
211.218511	4799.790643	7.269082	-0.042448	3.764687
211.627292	4807.868196	7.274086	-0.042530	3.767721
211.943353	4815.875371	7.279091	-0.042594	3.770725
212.196037	4823.906226	7.284096	-0.042646	3.773733
212.267288	4831.992021	7.289101	-0.042665	3.776755
212.644965	4839.903012	7.294106	-0.042740	3.779717
212.732600	4848.000801	7.299110	-0.042762	3.782739
212.746394	4855.998009	7.304115	-0.042770	3.785720
213.035548	4864.035686	7.309120	-0.042829	3.788720
213.090543	4872.117910	7.314125	-0.042845	3.791728
213.146527	4880.082207	7.319130	-0.042860	3.794691
213.576903	4888.131038	7.324134	-0.042946	3.797691
213.634710	4896.091065	7.329139	-0.042962	3.800647
213.687137	4904.120781	7.334144	-0.042977	3.803626
213.929073	4912.153505	7.339149	-0.043027	3.806609
214.290701	4920.136024	7.344154	-0.043100	3.809573
214.667062	4928.198353	7.349158	-0.043175	3.812564
214.720776	4936.227279	7.354163	-0.043190	3.815534
214.834668	4944.226109	7.359168	-0.043217	3.818492
215.119502	4952.270598	7.364173	-0.043275	3.821468
215.156381	4960.206775	7.369178	-0.043287	3.824396
215.539672	4968.310075	7.374182	-0.043364	3.827391
215.665915	4976.275715	7.379187	-0.043393	3.830328
215.846271	4984.349739	7.384192	-0.043431	3.833303
216.095942	4992.380411	7.389197	-0.043483	3.836262
216.232356	5000.329327	7.394202	-0.043514	3.839185
216.534789	5008.420658	7.399206	-0.043575	3.842163
216.522761	5016.347568	7.404211	-0.043578	3.845071
216.808406	5024.407291	7.409216	-0.043637	3.848031
217.291443	5032.418245	7.414221	-0.043732	3.850976
217.573395	5040.462696	7.419226	-0.043790	3.853926
217.869411	5048.508411	7.424230	-0.043850	3.856875
218.054803	5056.483501	7.429235	-0.043890	3.859793
218.424390	5064.557429	7.434240	-0.043964	3.862749
218.662334	5072.518100	7.439245	-0.044014	3.865659
218.709281	5080.586724	7.444250	-0.044028	3.868602
218.907805	5088.664599	7.449254	-0.044070	3.871549
218.948496	5096.903776	7.454259	-0.044083	3.874550
219.133180	5104.826700	7.459264	-0.044123	3.877436
219.528823	5112.761696	7.464269	-0.044202	3.880328
219.630667	5120.737104	7.469274	-0.044226	3.883227
219.894440	5128.743623	7.474278	-0.044280	3.886138
220.067282	5136.741193	7.479283	-0.044318	3.889042
220.490210	5144.755128	7.484288	-0.044402	3.891955
220.486347	5152.811952	7.489293	-0.044406	3.894873
220.768077	5160.829928	7.494298	-0.044464	3.897779
221.043001	5168.846595	7.499302	-0.044520	3.900684
221.223455	5176.810225	7.504307	-0.044559	3.903565
221.342997	5184.856441	7.509312	-0.044587	3.906472
221.522187	5192.874527	7.514317	-0.044625	3.909368
221.680885	5200.901411	7.519322	-0.044660	3.912265
221.944785	5208.946370	7.524326	-0.044715	3.915168
222.199336	5216.944970	7.529331	-0.044767	3.918053
222.505654	5224.959153	7.534336	-0.044830	3.920941
222.749729	5232.949461	7.539341	-0.044880	3.923818
222.762194	5240.997198	7.544346	-0.044888	3.926709
223.118371	5248.987826	7.549350	-0.044959	3.929583
223.031563	5257.052356	7.554355	-0.044949	3.932474
223.210303	5265.094125	7.559360	-0.044987	3.935359
223.468145	5273.088323	7.564365	-0.045040	3.938227
223.534898	5281.067187	7.569370	-0.045058	3.941084
223.792143	5289.089835	7.574374	-0.045111	3.943957
224.132590	5297.113575	7.579379	-0.045180	3.946830
224.203948	5305.138713	7.584384	-0.045198	3.949697
224.405940	5313.191496	7.589389	-0.045241	3.952574
224.595590	5321.214915	7.594394	-0.045282	3.955438
224.974413	5329.232659	7.599398	-0.045358	3.958301
225.132576	5337.202740	7.604403	-0.045392	3.961142
225.264426	5345.228130	7.609408	-0.045422	3.963999
225.611545	5353.276548	7.614413	-0.045492	3.966867
225.652133	5361.260815	7.619418	-0.045505	3.969704
225.997776	5369.334335	7.624422	-0.045575	3.972576
226.005635	5377.343159	7.629427	-0.045581	3.975417
226.310822	5385.351114	7.634432	-0.045643	3.978261
226.682132	5393.389243	7.639437	-0.045718	3.981114
226.762744	5401.383020	7.644442	-0.045738	3.983946
227.060299	5409.453031	7.649446	-0.045799	3.986805
227.076094	5417.425065	7.654451	-0.045807	3.989623
227.301088	5425.485298	7.659456	-0.045854	3.992474
227.463728	5433.531182	7.664461	-0.045890	3.995316
227.692314	5441.508214	7.669466	-0.045938	3.998134
227.762280	5449.564467	7.674470	-0.045956	4.000974
227.955237	5457.519083	7.679475	-0.045997	4.003779
227.992044	5465.558103	7.684480	-0.046009	4.006609
228.439235	5473.585754	7.689485	-0.046098	4.009440
228.472638	5481.601764	7.694490	-0.046109	4.012258
228.750911	5489.679499	7.699494	-0.046166	4.015099
228.814346	5497.678035	7.704499	-0.046183	4.017907
228.986174	5505.681104	7.709504	-0.046221	4.020717
229.232347	5513.700927	7.714509	-0.046272	4.023531
229.553668	5521.709900	7.719514	-0.046337	4.026341
229.686639	5529.721888	7.724518	-0.046367	4.029147
229.953519	5537.768700	7.729523	-0.046422	4.031965
230.340822	5545.885908	7.734528	-0.046499	4.034808
230.407890	5553.856963	7.739533	-0.046517	4.037593
230.631553	5561.810933	7.744538	-0.046564	4.040372
230.863049	5569.824781	7.749542	-0.046612	4.043170
231.166052	5577.827897	7.754547	-0.046674	4.045964
231.381617	5585.827712	7.759552	-0.046719	4.048753
231.485640	5593.891537	7.764557	-0.046744	4.051561
231.502205	5601.898109	7.769562	-0.046752	4.054346
231.760569	5609.945355	7.774566	-0.046806	4.057146
231.877925	5617.882555	7.779571	-0.046833	4.059904
232.319384	5625.923812	7.784576	-0.046920	4.062701
232.233722	5633.960290	7.789581	-0.046910	4.065488
232.304171	5641.983447	7.794586	-0.046928	4.068269
232.552916	5650.016822	7.799590	-0.046980	4.071055
232.813887	5658.045405	7.804595	-0.047034	4.073837
232.946010	5666.067471	7.809600	-0.047063	4.076614
233.045401	5674.040318	7.814605	-0.047087	4.079371
233.285733	5682.052039	7.819610	-0.047137	4.082141
233.650820	5690.064511	7.824614	-0.047210	4.084912
233.494241	5698.130617	7.829619	-0.047187	4.087692
233.980379	5706.086174	7.834624	-0.047282	4.090440
234.211159	5714.177552	7.839629	-0.047331	4.093231
234.190965	5722.199634	7.844634	-0.047332	4.095992
234.570265	5730.193087	7.849638	-0.047408	4.098746
234.883461	5738.210902	7.854643	-0.047472	4.101506
235.036804	5746.195638	7.859648	-0.047505	4.104251
234.947204	5754.272082	7.864653	-0.047494	4.107023
235.181846	5762.255568	7.869658	-0.047543	4.109764
235.480000	5770.334181	7.874662	-0.047604	4.112538
235.316349	5778.392300	7.879667	-0.047579	4.115296
235.541740	5786.391547	7.884672	-0.047626	4.118038
235.756762	5794.359171	7.889677	-0.047671	4.120766
235.842222	5802.345022	7.894682	-0.047692	4.123498
236.017793	5810.364088	7.899686	-0.047730	4.126240
236.428291	5818.418685	7.904691	-0.047812	4.128995
236.386777	5826.461769	7.909696	-0.047810	4.131739
236.739141	5834.486357	7.914701	-0.047880	4.134479
236.986634	5842.480657	7.919706	-0.047932	4.137207
237.115588	5850.547716	7.924710	-0.047961	4.139955
237.451178	5858.536931	7.929715	-0.048029	4.142678
237.623801	5866.522420	7.934720	-0.048066	4.145396
238.014286	5874.546266	7.939725	-0.048144	4.148127
238.004296	5882.594603	7.944730	-0.048148	4.150860
238.206649	5890.664128	7.949734	-0.048191	4.153601
238.657653	5898.680140	7.954739	-0.048280	4.156325
238.782472	5906.663588	7.959744	-0.048308	4.159033
238.953454	5914.691342	7.964749	-0.048345	4.161754
238.787655	5922.607225	7.969754	-0.048320	4.164432
239.221271	5930.710795	7.974758	-0.048406	4.167178
239.152050	5938.698530	7.979763	-0.048398	4.169877
239.417975	5946.711142	7.984768	-0.048453	4.172587
239.760348	5954.760861	7.989773	-0.048522	4.175309
239.843586	5962.745540	7.994778	-0.048543	4.178004
240.085943	5970.770217	7.999782	-0.048593	4.180712
240.237676	5978.780807	8.004787	-0.048627	4.183413
240.340439	5986.815792	8.009792	-0.048651	4.186120
240.668207	5994.809148	8.014797	-0.048717	4.188813
240.740614	6002.834230	8.019802	-0.048736	4.191512
241.259516	6010.987457	8.024806	-0.048838	4.194258
241.493391	6018.942909	8.029811	-0.048887	4.196932
241.604299	6026.896088	8.034816	-0.048913	4.199603
241.671521	6034.950661	8.039821	-0.048931	4.202305
241.835295	6042.866896	8.044826	-0.048966	4.204961
241.975388	6050.925017	8.049830	-0.048998	4.207661
242.306608	6058.942645	8.054835	-0.049065	4.210349
242.454838	6066.973689	8.059840	-0.049097	4.213037
242.562079	6075.016725	8.064845	-0.049123	4.215727
242.702707	6082.974261	8.069850	-0.049154	4.218388
243.086996	6091.001921	8.074854	-0.049231	4.221072
243.073959	6099.007789	8.079859	-0.049234	4.223743
243.161037	6107.062721	8.084864	-0.049255	4.226431
243.638622	6115.051898	8.089869	-0.049349	4.229098
243.817780	6123.086515	8.094874	-0.049388	4.231775
243.860404	6131.140398	8.099878	-0.049401	4.234457
243.950550	6139.194352	8.104883	-0.049423	4.237137
244.255987	6147.116058	8.109888	-0.049486	4.239773
244.426649	6155.182778	8.114893	-0.049523	4.242454
244.308127	6163.116655	8.119898	-0.049506	4.245087
244.675026	6171.225062	8.124902	-0.049579	4.247781
244.916791	6179.209292	8.129907	-0.049630	4.250431
245.100082	6187.275540	8.134912	-0.049669	4.253105
245.505641	6195.274197	8.139917	-0.049750	4.255758
245.675385	6203.296390	8.144922	-0.049787	4.258414
245.852739	6211.322529	8.149926	-0.049825	4.261070
245.956980	6219.309326	8.154931	-0.049850	4.263711
246.409734	6227.304597	8.159936	-0.049939	4.266356
246.572855	6235.385134	8.164941	-0.049975	4.269025
246.715156	6243.358678	8.169946	-0.050007	4.271657
246.785719	6251.483894	8.174950	-0.050025	4.274337
247.162856	6259.489209	8.179955	-0.050101	4.276978
247.270647	6267.412296	8.184960	-0.050126	4.279588
247.507359	6275.500377	8.189965	-0.050175	4.282251
247.564379	6283.415588	8.194970	-0.050191	4.284855
247.825472	6291.498972	8.199974	-0.050245	4.287514
248.100342	6299.508255	8.204979	-0.050302	4.290147
248.399945	6307.569567	8.209984	-0.050363	4.292796
248.595750	6315.593650	8.214989	-0.050404	4.295430
248.615354	6323.592498	8.219994	-0.050413	4.298053
248.891697	6331.570394	8.224998	-0.050470	4.300669
249.004382	6339.592243	8.230003	-0.050496	4.303297
249.298013	6347.615959	8.235008	-0.050556	4.305925
249.570176	6355.657593	8.240013	-0.050612	4.308557
249.687583	6363.662755	8.245018	-0.050639	4.311174
250.040108	6371.708831	8.250022	-0.050710	4.313805
250.156105	6379.712457	8.255027	-0.050737	4.316419
250.370715	6387.700695	8.260032	-0.050782	4.319027
250.609990	6395.707701	8.265037	-0.050832	4.321639
250.480694	6403.703427	8.270042	-0.050813	4.324244
250.916791	6411.779445	8.275046	-0.050900	4.326877
250.953007	6419.747897	8.280051	-0.050912	4.329471
250.842212	6427.801915	8.285056	-0.050896	4.332090
250.938587	6435.843137	8.290061	-0.050920	4.334705
251.231630	6443.794973	8.295066	-0.050979	4.337290
251.461343	6451.839497	8.300070	-0.051027	4.339903
251.569825	6459.864399	8.305075	-0.051053	4.342508
251.814408	6467.814491	8.310080	-0.051104	4.345088
251.883826	6475.907678	8.315085	-0.051122	4.347711
251.974975	6483.884856	8.320090	-0.051144	4.350296
252.209401	6491.997261	8.325094	-0.051193	4.352923
252.514061	6499.998489	8.330099	-0.051255	4.355513
252.604707	6507.969917	8.335104	-0.051277	4.358091
252.973954	6515.961328	8.340109	-0.051351	4.360676
253.207471	6523.936873	8.345114	-0.051400	4.363253
253.506661	6531.966381	8.350118	-0.051461	4.365846
253.690004	6539.972819	8.355123	-0.051500	4.368429
253.741068	6548.010605	8.360128	-0.051515	4.371020
253.897817	6556.115346	8.365133	-0.051550	4.373632
254.021681	6564.086859	8.370138	-0.051578	4.376200
254.045671	6572.067705	8.375142	-0.051588	4.378768
254.305991	6580.094960	8.380147	-0.051641	4.381351
254.446288	6588.064908	8.385152	-0.051673	4.383913
254.823756	6596.147537	8.390157	-0.051748	4.386511
255.019844	6604.128100	8.395162	-0.051790	4.389074
255.047556	6612.183250	8.400166	-0.051801	4.391658
255.256785	6620.226685	8.405171	-0.051845	4.394238
255.407013	6628.240767	8.410176	-0.051878	4.396807
255.649062	6636.233824	8.415181	-0.051928	4.399368
255.732041	6644.262336	8.420186	-0.051949	4.401938
256.075825	6652.200905	8.425190	-0.052018	4.404479
256.292757	6660.296504	8.430195	-0.052064	4.407068
256.368412	6668.254344	8.435200	-0.052083	4.409611
256.559340	6676.361870	8.440205	-0.052124	4.412201
256.794058	6684.338581	8.445210	-0.052173	4.414747
257.089188	6692.405326	8.450214	-0.052233	4.417321
257.108219	6700.343523	8.455219	-0.052242	4.419852
257.104331	6708.415012	8.460224	-0.052247	4.422423
257.437202	6716.387655	8.465229	-0.052314	4.424963
257.521408	6724.439926	8.470234	-0.052335	4.427525
257.951163	6732.426645	8.475238	-0.052420	4.430067
258.207411	6740.487154	8.480243	-0.052473	4.432630
258.328710	6748.480390	8.485248	-0.052501	4.435169
258.594954	6756.581738	8.490253	-0.052556	4.437742
258.831334	6764.472699	8.495258	-0.052605	4.440247
258.996199	6772.526650	8.500262	-0.052641	4.442801
258.866613	6780.507959	8.505267	-0.052622	4.445330
259.141761	6788.565020	8.510272	-0.052679	4.447883
259.584606	6796.569679	8.515277	-0.052767	4.450418
259.716358	6804.623027	8.520282	-0.052796	4.452966
259.755782	6812.617857	8.525286	-0.052809	4.455494
259.822677	6820.668347	8.530291	-0.052827	4.458038
259.930706	6828.628106	8.535296	-0.052852	4.460552
260.154763	6836.694104	8.540301	-0.052899	4.463099
260.280692	6844.622256	8.545306	-0.052928	4.465600
260.592588	6852.719469	8.550310	-0.052991	4.468154
260.791573	6860.725420	8.555315	-0.053033	4.470677
260.873950	6868.768831	8.560320	-0.053054	4.473211
261.596869	6876.739396	8.565325	-0.053194	4.475721
261.955737	6884.717080	8.570330	-0.053266	4.478232
262.442814	6892.763804	8.575335	-0.053362	4.480763
262.563561	6900.772774	8.580339	-0.053390	4.483279
262.691905	6908.774301	8.585344	-0.053419	4.485792
262.937517	6916.827154	8.590349	-0.053470	4.488320
263.168292	6924.815078	8.595354	-0.053518	4.490826
263.520964	6932.856400	8.600359	-0.053589	4.493348
263.600114	6940.908507	8.605363	-0.053609	4.495871
263.738397	6948.869980	8.610368	-0.053640	4.498364
264.116689	6956.926960	8.615373	-0.053716	4.500886
264.302456	6964.862201	8.620378	-0.053756	4.503368
264.304994	6972.894097	8.625383	-0.053761	4.505879
264.462768	6980.960411	8.630387	-0.053796	4.508400
264.658183	6988.976052	8.635392	-0.053838	4.510903
264.748959	6997.059948	8.640397	-0.053860	4.513426
265.043091	7005.060035	8.645402	-0.053920	4.515921
265.278096	7013.052004	8.650407	-0.053969	4.518413
265.513743	7021.010391	8.655411	-0.054018	4.520893
265.535247	7028.975458	8.660416	-0.054027	4.523373
265.658993	7037.040692	8.665421	-0.054056	4.525883
265.927283	7045.006284	8.670426	-0.054111	4.528361
266.069027	7053.034255	8.675431	-0.054143	4.530857
266.242210	7061.121849	8.680435	-0.054180	4.533370
266.427596	7069.143548	8.685440	-0.054220	4.535861
266.565471	7077.131711	8.690445	-0.054251	4.538340
266.671222	7085.091215	8.695450	-0.054276	4.540809
266.839765	7093.164651	8.700455	-0.054312	4.543312
266.934451	7101.149160	8.705459	-0.054335	4.545786
266.987968	7109.174520	8.710464	-0.054351	4.548271
267.248230	7117.240917	8.715469	-0.054404	4.550767
267.326598	7125.261968	8.720474	-0.054424	4.553248
267.420031	7133.312642	8.725479	-0.054447	4.555737
267.419693	7141.283132	8.730483	-0.054452	4.558200
267.809087	7149.267005	8.735488	-0.054530	4.560666
268.080524	7157.299163	8.740493	-0.054586	4.563145
268.233777	7165.309752	8.745498	-0.054619	4.565616
268.237932	7173.351400	8.750503	-0.054625	4.568095
268.373486	7181.336365	8.755507	-0.054656	4.570555
268.719122	7189.382124	8.760512	-0.054726	4.573033
268.795862	7197.404387	8.765517	-0.054745	4.575503
268.896151	7205.397490	8.770522	-0.054769	4.577962
269.025604	7213.404047	8.775527	-0.054798	4.580423
269.127232	7221.426174	8.780531	-0.054823	4.582888
269.454033	7229.418951	8.785536	-0.054889	4.585343
269.567664	7237.492562	8.790541	-0.054915	4.587821
269.622530	7245.484087	8.795546	-0.054931	4.590273
269.962479	7253.560336	8.800551	-0.054999	4.592749
270.060226	7261.523883	8.805555	-0.055023	4.595190
270.379964	7269.550901	8.810560	-0.055088	4.597649
270.479257	7277.529203	8.815565	-0.055111	4.600091
270.609084	7285.563865	8.820570	-0.055141	4.602549
270.810992	7293.580477	8.825575	-0.055184	4.605001
271.035245	7301.628036	8.830579	-0.055231	4.607460
271.349753	7309.585029	8.835584	-0.055294	4.609891
271.553857	7317.655639	8.840589	-0.055338	4.612354
271.592414	7325.658743	8.845594	-0.055350	4.614796
271.623781	7333.687599	8.850599	-0.055361	4.617245
271.851409	7341.668885	8.855603	-0.055409	4.619678
272.048230	7349.664658	8.860608	-0.055451	4.622113
272.414357	7357.686680	8.865613	-0.055524	4.624556
272.507182	7365.716484	8.870618	-0.055547	4.626999
272.766421	7373.723325	8.875623	-0.055600	4.629435
272.797329	7381.740993	8.880627	-0.055611	4.631872
273.005878	7389.776836	8.885632	-0.055655	4.634313
273.314588	7397.870822	8.890637	-0.055718	4.636771
273.266899	7405.769371	8.895642	-0.055715	4.639168
273.727854	7413.824223	8.900647	-0.055806	4.641611
274.045810	7421.776849	8.905651	-0.055870	4.644022
274.196713	7429.852577	8.910656	-0.055904	4.646469
274.463912	7437.868184	8.915661	-0.055959	4.648897
274.545299	7445.880019	8.920666	-0.055979	4.651322
274.919550	7453.878898	8.925671	-0.056054	4.653741
274.938975	7461.898913	8.930675	-0.056063	4.656166
275.046851	7469.910152	8.935680	-0.056088	4.658588
275.320607	7477.953378	8.940685	-0.056144	4.661017
275.489203	7485.921721	8.945690	-0.056181	4.663422
275.445019	7493.941662	8.950695	-0.056178	4.665842
275.602568	7502.012520	8.955699	-0.056213	4.668276
275.686651	7509.995007	8.960704	-0.056234	4.670682
276.034690	7518.095270	8.965709	-0.056304	4.673122
276.195403	7526.130238	8.970714	-0.056339	4.675542
276.339709	7534.099810	8.975719	-0.056371	4.677940
276.346302	7542.080884	8.980723	-0.056378	4.680341
276.390307	7550.069449	8.985728	-0.056391	4.682742
276.974558	7558.040126	8.990733	-0.056505	4.685136
276.940754	7566.081158	8.995738	-0.056504	4.687552
277.007167	7574.089658	9.000743	-0.056522	4.689956
277.306110	7582.174919	9.005747	-0.056583	4.692381
277.150039	7590.118126	9.010752	-0.056559	4.694763
277.479440	7598.176667	9.015757	-0.056625	4.697178
277.706727	7606.128125	9.020762	-0.056673	4.699559
278.034720	7614.199316	9.025767	-0.056739	4.701975
278.077102	7622.150158	9.030771	-0.056752	4.704354
278.076926	7630.209064	9.035776	-0.056758	4.706765
278.480360	7638.230950	9.040781	-0.056838	4.709162
278.589979	7646.215626	9.045786	-0.056864	4.711547
278.713417	7654.309098	9.050791	-0.056892	4.713964
278.767408	7662.348553	9.055795	-0.056907	4.716364
278.847496	7670.282489	9.060800	-0.056928	4.718730
279.076572	7678.306806	9.065805	-0.056975	4.721123
279.242767	7686.287480	9.070810	-0.057012	4.723501
279.328976	7694.343728	9.075815	-0.057033	4.725900
279.530933	7702.399078	9.080819	-0.057076	4.728298
279.694714	7710.358488	9.085824	-0.057112	4.730666
280.071276	7718.482895	9.090829	-0.057187	4.733081
280.103783	7726.440636	9.095834	-0.057198	4.735447
280.256500	7734.432156	9.100839	-0.057232	4.737821
280.465003	7742.473628	9.105843	-0.057276	4.740208
280.504455	7750.453029	9.110848	-0.057289	4.742576
280.684764	7758.450798	9.115853	-0.057328	4.744948
280.789731	7766.476984	9.120858	-0.057352	4.747328
281.087753	7774.488615	9.125863	-0.057413	4.749701
281.110135	7782.547220	9.130867	-0.057423	4.752088
281.220691	7790.578347	9.135872	-0.057448	4.754466
281.540360	7798.587821	9.140877	-0.057513	4.756835
281.498419	7806.565944	9.145882	-0.057511	4.759195
281.718990	7814.587511	9.150887	-0.057557	4.761565
281.983543	7822.542968	9.155891	-0.057612	4.763915
282.233150	7830.592129	9.160896	-0.057663	4.766291
282.549107	7838.644240	9.165901	-0.057727	4.768667
282.603470	7846.652270	9.170906	-0.057743	4.771029
282.899133	7854.709125	9.175911	-0.057803	4.773404
283.157745	7862.737780	9.180915	-0.057857	4.775769
282.979409	7870.680223	9.185920	-0.057829	4.778109
283.158479	7878.747533	9.190925	-0.057867	4.780484
283.191135	7886.699958	9.195930	-0.057879	4.782824
283.408160	7894.679344	9.200935	-0.057924	4.785170
283.396844	7902.732419	9.205939	-0.057927	4.787538
283.870853	7910.710105	9.210944	-0.058021	4.789880
283.766200	7918.798409	9.215949	-0.058007	4.792256
283.912007	7926.810764	9.220954	-0.058039	4.794608
284.335262	7934.873223	9.225959	-0.058123	4.796972
284.406936	7942.763566	9.230963	-0.058142	4.799285
284.474829	7950.798307	9.235968	-0.058160	4.801640
284.709844	7958.839896	9.240973	-0.058209	4.803995
284.886964	7966.872794	9.245978	-0.058247	4.806347
285.008144	7974.892717	9.250983	-0.058275	4.808693
285.224588	7982.925776	9.255987	-0.058320	4.811042
285.316378	7990.270740	9.260992	-0.058342	4.813190
285.568463	7994.782424	9.265997	-0.058392	4.814507

285.575715	7997.245998	9.271002	-0.058395	4.815227
285.523136	7998.562382	9.276007	-0.058386	4.815612
285.635927	7999.001431	9.281011	-0.058408	4.815740
285.618001	7999.968102	9.286016	-0.058405	4.816022
285.948654	7999.981597	9.291021	-0.058467	4.816025
286.009166	7999.945303	9.296026	-0.058478	4.816014
286.107566	7999.982358	9.301031	-0.058496	4.816024
286.184290	8000.007265	9.306035	-0.058511	4.816031
286.307210	7999.955009	9.311040	-0.058534	4.816015
286.464276	7999.952526	9.316045	-0.058563	4.816013
286.433107	7999.949827	9.321050	-0.058557	4.816013
286.494604	7999.961635	9.326055	-0.058569	4.816016
286.716667	8000.004145	9.331059	-0.058610	4.816027
286.698058	7999.953589	9.336064	-0.058607	4.816012
286.911143	7999.993799	9.341069	-0.058646	4.816023
286.902418	7999.941285	9.346074	-0.058645	4.816008
286.885425	7999.907855	9.351079	-0.058642	4.815998
286.901792	7999.961585	9.356083	-0.058645	4.816014
286.858296	7999.985375	9.361088	-0.058637	4.816021
286.895950	8000.012779	9.366093	-0.058644	4.816029
286.690327	7999.987672	9.371098	-0.058605	4.816022
286.767945	8000.041448	9.376103	-0.058620	4.816038
286.911179	8000.023754	9.381107	-0.058647	4.816032
286.896365	8000.011735	9.386112	-0.058644	4.816028
287.119075	8000.004036	9.391117	-0.058685	4.816025
287.076155	7999.900677	9.396122	-0.058677	4.815995
287.211998	7999.898877	9.401127	-0.058703	4.815994
287.277727	7999.928929	9.406131	-0.058715	4.816002
287.230638	7999.878922	9.411136	-0.058706	4.815988
287.320978	7999.973535	9.416141	-0.058723	4.816015
287.246708	7999.957229	9.421146	-0.058709	4.816010
287.557933	7999.877408	9.426151	-0.058767	4.815985
287.520429	7999.985725	9.431155	-0.058761	4.816017
287.149808	7999.968302	9.436160	-0.058692	4.816014
287.363035	8000.020271	9.441165	-0.058731	4.816028
287.393758	7999.977022	9.446170	-0.058737	4.816015
287.339091	8000.003815	9.451175	-0.058727	4.816024
287.241084	7999.958225	9.456179	-0.058709	4.816011
287.429260	7999.944555	9.461184	-0.058744	4.816006
287.570593	8000.058263	9.466189	-0.058770	4.816038
287.493299	8000.015186	9.471194	-0.058756	4.816026
287.445409	8000.021800	9.476199	-0.058747	4.816028
287.560965	8000.022837	9.481203	-0.058769	4.816028
287.464375	7999.968724	9.486208	-0.058751	4.816013
287.785885	7999.989537	9.491213	-0.058811	4.816017
287.899995	7999.999098	9.496218	-0.058832	4.816019
287.780952	7999.953124	9.501223	-0.058810	4.816006
287.747796	8000.001680	9.506227	-0.058804	4.816021
287.760387	7999.884370	9.511232	-0.058806	4.815986
287.818261	7999.965571	9.516237	-0.058817	4.816010
287.746937	7999.953591	9.521242	-0.058804	4.816007
287.683007	8000.014411	9.526247	-0.058792	4.816025
287.655349	8000.049175	9.531251	-0.058787	4.816035
287.543622	8000.023638	9.536256	-0.058766	4.816028
287.523587	8000.058541	9.541261	-0.058762	4.816039
287.351368	8000.025492	9.546266	-0.058730	4.816030
287.617741	7999.975845	9.551271	-0.058780	4.816014
287.593140	7999.982881	9.556275	-0.058775	4.816016
287.977365	7999.989876	9.561280	-0.058847	4.816016
288.274021	8000.045502	9.566285	-0.058902	4.816031
288.020461	7999.958611	9.571290	-0.058855	4.816007
288.061214	8000.013855	9.576295	-0.058863	4.816023
288.277005	7999.992139	9.581299	-0.058903	4.816015
288.100759	7999.949399	9.586304	-0.058870	4.816004
287.970582	8000.000464	9.591309	-0.058846	4.816019
288.211806	7999.980280	9.596314	-0.058891	4.816012
288.264183	7999.978032	9.601319	-0.058901	4.816011
287.990553	7999.981606	9.606323	-0.058850	4.816014
287.874264	7999.979495	9.611328	-0.058828	4.816014
288.071029	8000.041852	9.616333	-0.058865	4.816031
287.943752	8000.005345	9.621338	-0.058841	4.816021
287.986727	7999.994377	9.626343	-0.058849	4.816017
288.213592	8000.027361	9.631347	-0.058891	4.816026
288.206423	7999.964188	9.636352	-0.058890	4.816007
288.352734	8000.077989	9.641357	-0.058917	4.816040
288.369407	8000.014181	9.646362	-0.058921	4.816021
288.399434	8000.005114	9.651367	-0.058926	4.816018
288.215812	8000.011394	9.656371	-0.058892	4.816021
288.163469	7999.980525	9.661376	-0.058882	4.816012
288.358041	7999.995825	9.666381	-0.058919	4.816016
288.213122	7999.932282	9.671386	-0.058892	4.815998
288.334875	7999.929159	9.676391	-0.058914	4.815996
288.305484	8000.017322	9.681395	-0.058909	4.816022
288.263754	7999.925736	9.686400	-0.058901	4.815996
288.235666	7999.978659	9.691405	-0.058896	4.816011
288.108853	7999.996660	9.696410	-0.058872	4.816017
288.429929	8000.044182	9.701415	-0.058932	4.816030
288.373031	8000.064523	9.706419	-0.058922	4.816036
288.209356	8000.023079	9.711424	-0.058891	4.816025
288.450472	8000.011442	9.716429	-0.058936	4.816020
288.574238	8000.031865	9.721434	-0.058959	4.816025
288.547627	8000.036728	9.726439	-0.058954	4.816027
288.384794	8000.024152	9.731443	-0.058924	4.816024
288.309308	7999.988587	9.736448	-0.058910	4.816014
288.386429	8000.049837	9.741453	-0.058925	4.816031
288.352113	8000.010747	9.746458	-0.058918	4.816020
288.371321	8000.031404	9.751463	-0.058922	4.816026
288.316695	8000.038963	9.756467	-0.058912	4.816029
288.217423	7999.965565	9.761472	-0.058893	4.816008
288.474515	8000.067490	9.766477	-0.058941	4.816036
288.297393	7999.998018	9.771482	-0.058908	4.816017
288.286127	8000.020258	9.776487	-0.058906	4.816023
288.341527	8000.059740	9.781491	-0.058917	4.816035
288.292436	8000.042822	9.786496	-0.058908	4.816030
288.202942	8000.004865	9.791501	-0.058891	4.816019
288.283132	8000.005260	9.796506	-0.058906	4.816019
288.481300	8000.033449	9.801511	-0.058943	4.816026
288.497199	8000.026262	9.806515	-0.058946	4.816024
288.468729	7999.993690	9.811520	-0.058941	4.816015
288.533107	8000.050434	9.816525	-0.058953	4.816031
288.500243	8000.060526	9.821530	-0.058947	4.816034
288.503688	7999.996477	9.826535	-0.058947	4.816015
288.439481	8000.031645	9.831539	-0.058935	4.816026
288.509746	7999.955988	9.836544	-0.058948	4.816003
288.588005	8000.006573	9.841549	-0.058963	4.816018
288.568520	7999.974164	9.846554	-0.058959	4.816008
288.584805	7999.946681	9.851559	-0.058962	4.816000
288.820625	8000.033260	9.856563	-0.059006	4.816024
288.433197	7999.930039	9.861568	-0.058934	4.815996
288.554541	8000.028426	9.866573	-0.058957	4.816024
288.741950	7999.949558	9.871578	-0.058992	4.816000
288.618696	7999.946251	9.876583	-0.058969	4.816000
288.848117	8000.019890	9.881587	-0.059012	4.816020
288.698323	7999.949846	9.886592	-0.058984	4.816000
288.730097	8000.025231	9.891597	-0.058990	4.816022
288.516712	7999.972196	9.896602	-0.058950	4.816008
288.629618	8000.019137	9.901607	-0.058971	4.816021
288.853582	8000.005051	9.906611	-0.059013	4.816016
288.789903	7999.964358	9.911616	-0.059001	4.816004
288.715810	8000.069875	9.916621	-0.058988	4.816035
288.785674	8000.026269	9.921626	-0.059001	4.816022
288.492509	8000.012389	9.926631	-0.058946	4.816020
288.560719	8000.037144	9.931635	-0.058959	4.816027
288.651320	7999.959720	9.936640	-0.058976	4.816004
288.637501	8000.022521	9.941645	-0.058973	4.816022
288.609259	7999.909807	9.946650	-0.058968	4.815989
288.600762	7999.911794	9.951655	-0.058966	4.815990
288.849897	7999.936636	9.956659	-0.059013	4.815996
288.593479	7999.977924	9.961664	-0.058965	4.816009
288.795827	8000.001914	9.966669	-0.059003	4.816015
288.772836	7999.998294	9.971674	-0.058999	4.816014
288.775333	7999.950257	9.976679	-0.058999	4.816000
288.854180	8000.042528	9.981683	-0.059014	4.816027
288.781182	7999.992048	9.986688	-0.059000	4.816012
289.014840	8000.045461	9.991693	-0.059044	4.816027
289.043179	8000.039570	9.996698	-0.059049	4.816025
288.796729	7999.994481	10.001703	-0.059003	4.816013
288.855475	7999.976319	10.006707	-0.059014	4.816007
288.841791	7999.940810	10.011712	-0.059012	4.815997
289.020439	7999.984673	10.016717	-0.059045	4.816009
288.938060	8000.009894	10.021722	-0.059030	4.816017
288.828204	7999.951262	10.026727	-0.059009	4.816000
288.853541	7999.979512	10.031731	-0.059014	4.816008
288.864171	7999.980778	10.036736	-0.059016	4.816009
289.100882	7999.977610	10.041741	-0.059060	4.816006
288.937510	8000.036621	10.046746	-0.059030	4.816025
288.939772	8000.003539	10.051751	-0.059030	4.816015
289.111815	8000.003469	10.056755	-0.059062	4.816014
288.974505	8000.034101	10.061760	-0.059037	4.816024
289.103233	8000.051410	10.066765	-0.059061	4.816028
289.071687	8000.029467	10.071770	-0.059055	4.816022
288.872493	7999.993787	10.076775	-0.059018	4.816012
288.925412	8000.053529	10.081779	-0.059028	4.816030
289.030911	7999.948592	10.086784	-0.059048	4.815998
289.098470	8000.039590	10.091789	-0.059060	4.816025
288.963518	8000.025383	10.096794	-0.059035	4.816021
289.070020	7999.978169	10.101799	-0.059055	4.816007
289.271594	8000.006421	10.106803	-0.059093	4.816014
289.034141	7999.958290	10.111808	-0.059048	4.816001
289.170575	7999.982150	10.116813	-0.059074	4.816007
289.279776	8000.009789	10.121818	-0.059094	4.816015
289.267065	7999.973229	10.126823	-0.059092	4.816004
289.164185	8000.032272	10.131827	-0.059073	4.816022
289.205356	8000.005241	10.136832	-0.059081	4.816014
289.225077	7999.976752	10.141837	-0.059084	4.816005
289.175020	8000.011109	10.146842	-0.059075	4.816016
289.128014	8000.034836	10.151847	-0.059066	4.816023
289.307407	8000.082989	10.156851	-0.059100	4.816036
289.218325	8000.024734	10.161856	-0.059083	4.816020
289.152760	8000.043849	10.166861	-0.059071	4.816025
289.017691	8000.040326	10.171866	-0.059046	4.816025
288.991238	8000.030231	10.176871	-0.059041	4.816022
288.929378	7999.993845	10.181875	-0.059030	4.816012
288.928721	7999.993837	10.186880	-0.059029	4.816012
289.029561	8000.067275	10.191885	-0.059048	4.816033
289.117183	8000.017580	10.196890	-0.059065	4.816018
289.102466	7999.992738	10.201895	-0.059062	4.816011
289.353275	8000.048602	10.206899	-0.059109	4.816026
289.249669	7999.993289	10.211904	-0.059089	4.816010
289.181114	8000.028379	10.216909	-0.059077	4.816021
289.071164	8000.018902	10.221914	-0.059056	4.816019
289.290611	7999.955577	10.226919	-0.059097	4.815999
289.091417	7999.987220	10.231923	-0.059060	4.816009
289.148535	7999.962617	10.236928	-0.059071	4.816002
289.294958	7999.992002	10.241933	-0.059098	4.816010
289.102313	8000.008804	10.246938	-0.059062	4.816015
288.909582	7999.952938	10.251943	-0.059026	4.816000
289.237150	8000.016610	10.256947	-0.059088	4.816017
289.076072	7999.936742	10.261952	-0.059058	4.815995
289.190314	8000.013629	10.266957	-0.059079	4.816016
289.265766	8000.035311	10.271962	-0.059093	4.816022
289.180946	7999.979271	10.276967	-0.059077	4.816006
289.087153	8000.024588	10.281971	-0.059060	4.816020
289.162923	7999.977883	10.286976	-0.059074	4.816006
289.351832	8000.024071	10.291981	-0.059109	4.816019
289.476365	8000.012451	10.296986	-0.059132	4.816015
289.169761	7999.990844	10.301991	-0.059075	4.816010
289.360894	8000.060583	10.306995	-0.059111	4.816029
289.397204	7999.970415	10.312000	-0.059118	4.816003
289.223054	8000.002513	10.317005	-0.059085	4.816013
289.321608	8000.055606	10.322010	-0.059104	4.816028
289.203223	8000.023534	10.327015	-0.059082	4.816019
289.223056	8000.090154	10.332019	-0.059086	4.816039
289.220999	8000.055925	10.337024	-0.059085	4.816029
289.367357	8000.051113	10.342029	-0.059113	4.816026
289.509270	8000.051564	10.347034	-0.059139	4.816026
289.362297	7999.983706	10.352039	-0.059112	4.816007
289.349597	8000.056146	10.357043	-0.059109	4.816028
289.307946	8000.039362	10.362048	-0.059102	4.816023
289.499816	8000.003320	10.367053	-0.059137	4.816012
289.394466	8000.034534	10.372058	-0.059118	4.816021
289.283716	8000.051758	10.377063	-0.059097	4.816027
289.409529	8000.093592	10.382067	-0.059121	4.816039
289.314320	8000.049118	10.387072	-0.059103	4.816026
289.332813	8000.034498	10.392077	-0.059107	4.816022
289.547991	8000.045900	10.397082	-0.059147	4.816024
289.405636	7999.983470	10.402087	-0.059120	4.816006
289.581672	8000.062552	10.407091	-0.059153	4.816029
289.439002	8000.030037	10.412096	-0.059127	4.816020
289.455568	8000.049578	10.417101	-0.059130	4.816025
289.190886	8000.049038	10.422106	-0.059080	4.816027
289.529887	8000.064832	10.427111	-0.059144	4.816030
289.577908	8000.087083	10.432115	-0.059153	4.816036
289.300150	8000.094854	10.437120	-0.059101	4.816040
289.424765	8000.089647	10.442125	-0.059124	4.816037
289.463658	8000.047614	10.447130	-0.059131	4.816025
289.439888	8000.004440	10.452135	-0.059127	4.816012
289.519961	8000.067883	10.457139	-0.059142	4.816030
289.478932	8000.015846	10.462144	-0.059134	4.816015
289.382234	8000.045080	10.467149	-0.059116	4.816025
289.451466	8000.039933	10.472154	-0.059129	4.816023
289.435065	7999.972315	10.477159	-0.059126	4.816003
289.515891	8000.060350	10.482163	-0.059141	4.816028
289.332456	8000.043123	10.487168	-0.059107	4.816024
289.324628	8000.070769	10.492173	-0.059106	4.816032
289.417602	8000.056437	10.497178	-0.059123	4.816028
289.640601	8000.018824	10.502183	-0.059165	4.816015
289.727590	8000.089874	10.507187	-0.059181	4.816036
289.327962	8000.096494	10.512192	-0.059107	4.816040
289.554819	8000.086737	10.517197	-0.059149	4.816036
289.425915	8000.066227	10.522202	-0.059125	4.816030
289.645665	8000.036036	10.527207	-0.059166	4.816020
289.421468	8000.040508	10.532211	-0.059124	4.816023
289.415149	8000.033985	10.537216	-0.059123	4.816021
289.558431	8000.054765	10.542221	-0.059150	4.816026
289.526017	8000.041356	10.547226	-0.059144	4.816023
289.461780	7999.950425	10.552231	-0.059132	4.815996
289.562448	8000.058057	10.557235	-0.059151	4.816027
289.381090	8000.008808	10.562240	-0.059117	4.816014
289.587211	8000.055311	10.567245	-0.059156	4.816026
289.490936	8000.068523	10.572250	-0.059138	4.816031
289.526517	7999.999714	10.577255	-0.059144	4.816010
289.730254	8000.023732	10.582259	-0.059182	4.816016
289.560553	8000.027058	10.587264	-0.059151	4.816018
289.576629	8000.036973	10.592269	-0.059154	4.816021
289.555804	7999.990647	10.597274	-0.059150	4.816008
289.574390	7999.911911	10.602279	-0.059153	4.815985
289.721729	7999.926352	10.607283	-0.059181	4.815988
289.498528	7999.960764	10.612288	-0.059139	4.815999
289.742626	8000.025056	10.617293	-0.059185	4.816017
289.710788	8000.019137	10.622298	-0.059179	4.816015
289.620759	7999.984375	10.627303	-0.059162	4.816005
289.638391	8000.021034	10.632307	-0.059166	4.816016
289.480112	7999.987166	10.637312	-0.059136	4.816007
289.663622	8000.034325	10.642317	-0.059170	4.816020
289.594139	8000.042682	10.647322	-0.059157	4.816023
289.546242	8000.021511	10.652327	-0.059149	4.816017
289.688024	8000.081803	10.657331	-0.059175	4.816034
289.538450	8000.053436	10.662336	-0.059147	4.816026
289.869106	8000.103276	10.667341	-0.059209	4.816039
289.699301	8000.084159	10.672346	-0.059177	4.816034
289.611618	8000.060125	10.677351	-0.059161	4.816028
289.650833	8000.053363	10.682355	-0.059168	4.816025
289.572113	8000.020943	10.687360	-0.059154	4.816016
289.726002	8000.050465	10.692365	-0.059182	4.816024
289.630123	8000.032695	10.697370	-0.059165	4.816020
289.689745	7999.988902	10.702375	-0.059176	4.816006
289.699226	8000.033961	10.707379	-0.059178	4.816020
289.744630	8000.025175	10.712384	-0.059186	4.816017
289.806714	8000.033790	10.717389	-0.059198	4.816019
289.676481	8000.048521	10.722394	-0.059173	4.816024
289.724119	7999.992755	10.727399	-0.059182	4.816007
289.851328	8000.047439	10.732403	-0.059206	4.816023
289.868594	7999.994325	10.737408	-0.059209	4.816007
289.752784	8000.005045	10.742413	-0.059188	4.816011
289.881404	8000.060823	10.747418	-0.059212	4.816026
289.716939	8000.020431	10.752423	-0.059181	4.816015
289.864330	8000.094718	10.757427	-0.059209	4.816036
289.665002	8000.045141	10.762432	-0.059172	4.816023
289.777982	8000.063232	10.767437	-0.059193	4.816028
289.790173	8000.060252	10.772442	-0.059195	4.816027
289.736823	7999.972725	10.777447	-0.059185	4.816001
289.771498	8000.005420	10.782451	-0.059192	4.816011
289.834558	7999.989475	10.787456	-0.059203	4.816006
289.955547	8000.024810	10.792461	-0.059226	4.816015
289.988523	7999.996561	10.797466	-0.059232	4.816007
289.936330	8000.012713	10.802471	-0.059223	4.816012
289.930220	8000.051078	10.807475	-0.059221	4.816023
289.859626	8000.040179	10.812480	-0.059208	4.816020
289.915467	8000.013415	10.817485	-0.059219	4.816012
289.901293	7999.998200	10.822490	-0.059216	4.816008
289.801025	7999.984624	10.827495	-0.059198	4.816005
289.890795	8000.054656	10.832499	-0.059214	4.816025
289.750113	7999.963402	10.837504	-0.059188	4.815999
289.645676	7999.973260	10.842509	-0.059169	4.816002
289.711185	7999.976594	10.847514	-0.059181	4.816003
289.746877	7999.987934	10.852519	-0.059188	4.816006
289.589097	8000.088724	10.857523	-0.059158	4.816036
289.630362	8000.005057	10.862528	-0.059166	4.816011
289.853660	8000.039049	10.867533	-0.059208	4.816020
289.753381	7999.961354	10.872538	-0.059189	4.815998
289.757705	7999.960369	10.877543	-0.059190	4.815998
289.896081	7999.968236	10.882547	-0.059216	4.815999
289.917560	8000.013514	10.887552	-0.059220	4.816012
289.803809	8000.027477	10.892557	-0.059199	4.816017
289.821893	8000.002163	10.897562	-0.059202	4.816010
290.167126	7999.989218	10.902567	-0.059266	4.816004
290.126373	8000.045118	10.907571	-0.059259	4.816020
289.748649	7999.976264	10.912576	-0.059189	4.816002
289.842277	8000.036748	10.917581	-0.059206	4.816020
289.919548	8000.017855	10.922586	-0.059221	4.816014
289.960412	7999.928837	10.927591	-0.059228	4.815987
290.075017	7999.999322	10.932595	-0.059250	4.816007
290.035451	7999.993262	10.937600	-0.059242	4.816006
289.878497	8000.022468	10.942605	-0.059213	4.816015
289.754903	8000.034114	10.947610	-0.059190	4.816019
289.833371	7999.987459	10.952615	-0.059205	4.816005
289.983401	8000.019048	10.957619	-0.059233	4.816014
289.900367	8000.014334	10.962624	-0.059217	4.816013
289.987004	8000.051182	10.967629	-0.059233	4.816023
289.965558	8000.047590	10.972634	-0.059230	4.816022
289.819577	8000.010739	10.977639	-0.059202	4.816012
289.858122	8000.053122	10.982643	-0.059210	4.816024
289.918888	8000.041409	10.987648	-0.059221	4.816020
289.851961	8000.045538	10.992653	-0.059209	4.816022
289.602747	8000.064515	10.997658	-0.059162	4.816029
289.823916	8000.033281	11.002663	-0.059203	4.816019
289.790707	8000.059397	11.007667	-0.059197	4.816026
289.550916	8000.028319	11.012672	-0.059153	4.816019
289.780895	8000.069913	11.017677	-0.059196	4.816030
289.836336	8000.075202	11.022682	-0.059206	4.816031
289.734623	8000.025265	11.027687	-0.059187	4.816017
289.824741	8000.033322	11.032691	-0.059204	4.816019
290.050337	8000.009650	11.037696	-0.059246	4.816010
290.084567	7999.997454	11.042701	-0.059252	4.816007
290.157044	8000.023357	11.047706	-0.059266	4.816014
290.080072	8000.060431	11.052711	-0.059252	4.816025
290.132778	8000.098798	11.057715	-0.059261	4.816036
289.941966	8000.018384	11.062720	-0.059226	4.816014
289.930105	8000.075880	11.067725	-0.059224	4.816030
290.247416	8000.083800	11.072730	-0.059283	4.816031
289.819719	8000.033270	11.077735	-0.059203	4.816019
289.834668	8000.095528	11.082739	-0.059206	4.816037
290.021167	7999.969622	11.087744	-0.059241	4.815999
289.921899	8000.029800	11.092749	-0.059222	4.816017
289.971367	7999.997577	11.097754	-0.059232	4.816007
290.111266	7999.914637	11.102759	-0.059258	4.815982
290.257333	8000.008137	11.107763	-0.059285	4.816009
289.936508	7999.977720	11.112768	-0.059225	4.816002
290.196205	8000.001689	11.117773	-0.059274	4.816007
290.131096	8000.002645	11.122778	-0.059262	4.816008
290.035634	7999.970989	11.127783	-0.059244	4.815999
289.997355	8000.008767	11.132787	-0.059237	4.816010
289.959364	8000.039071	11.137792	-0.059230	4.816020
290.198178	8000.048767	11.142797	-0.059274	4.816021
290.137254	8000.066898	11.147802	-0.059263	4.816027
290.172512	8000.015180	11.152807	-0.059270	4.816011
290.230831	8000.021590	11.157811	-0.059281	4.816013
289.957950	7999.983497	11.162816	-0.059230	4.816003
290.126542	8000.011150	11.167821	-0.059261	4.816010
290.283806	8000.041803	11.172826	-0.059291	4.816019
290.215184	8000.073686	11.177831	-0.059278	4.816028
290.097214	8000.110014	11.182835	-0.059256	4.816040
290.013409	8000.056128	11.187840	-0.059240	4.816024
290.130214	8000.044367	11.192845	-0.059262	4.816020
290.085584	8000.062794	11.197850	-0.059254	4.816026
290.019540	8000.031673	11.202855	-0.059242	4.816017
290.180330	8000.035674	11.207859	-0.059272	4.816017
290.031953	8000.024428	11.212864	-0.059244	4.816015
290.243710	8000.055004	11.217869	-0.059284	4.816023
290.265698	8000.014800	11.222874	-0.059288	4.816011
290.177683	8000.018545	11.227879	-0.059271	4.816012
290.334000	7999.997886	11.232883	-0.059300	4.816005
290.169034	7999.988474	11.237888	-0.059270	4.816004
290.389795	7999.991430	11.242893	-0.059311	4.816003
290.273715	8000.049165	11.247898	-0.059289	4.816021
290.163904	8000.007629	11.252903	-0.059269	4.816009
290.217923	8000.044952	11.257907	-0.059279	4.816020
289.939982	8000.007835	11.262912	-0.059227	4.816010
290.008305	8000.015495	11.267917	-0.059240	4.816012
290.102274	8000.046064	11.272922	-0.059258	4.816021
290.224614	7999.979903	11.277927	-0.059280	4.816001
290.409807	8000.032438	11.282931	-0.059315	4.816015
290.051764	7999.991725	11.287936	-0.059248	4.816005
290.316068	8000.024328	11.292941	-0.059298	4.816013
290.431238	8000.060626	11.297946	-0.059319	4.816023
290.319129	8000.016911	11.302951	-0.059298	4.816011
290.397017	8000.076042	11.307955	-0.059313	4.816028
290.381229	8000.035150	11.312960	-0.059310	4.816016
290.399572	8000.025870	11.317965	-0.059313	4.816013
290.443076	8000.058726	11.322970	-0.059322	4.816023
290.195575	7999.992241	11.327975	-0.059275	4.816005
290.075008	7999.992187	11.332979	-0.059253	4.816005
290.299942	8000.008043	11.337984	-0.059295	4.816009
290.554392	8000.049016	11.342989	-0.059342	4.816019
290.313553	8000.062801	11.347994	-0.059298	4.816025
290.324112	8000.054448	11.352999	-0.059300	4.816022
290.404238	8000.087972	11.358003	-0.059315	4.816031
290.379686	8000.081117	11.363008	-0.059310	4.816030
290.301887	8000.062606	11.368013	-0.059296	4.816025
290.359865	8000.009165	11.373018	-0.059306	4.816009
290.389462	8000.018257	11.378023	-0.059312	4.816011
290.458870	8000.037693	11.383027	-0.059325	4.816016
290.520295	7999.980040	11.388032	-0.059336	4.815999
290.451437	7999.981996	11.393037	-0.059324	4.816000
290.488297	8000.011525	11.398042	-0.059331	4.816009
290.355755	7999.997361	11.403047	-0.059306	4.816005
290.478065	8000.014554	11.408051	-0.059329	4.816010
290.221014	7999.974611	11.413056	-0.059281	4.815999
290.276070	8000.000197	11.418061	-0.059291	4.816006
290.323906	8000.014965	11.423066	-0.059300	4.816010
290.472948	7999.999517	11.428071	-0.059328	4.816005
290.491441	8000.014819	11.433075	-0.059332	4.816010
290.287453	7999.964088	11.438080	-0.059294	4.815996
290.429366	7999.957058	11.443085	-0.059320	4.815993
290.395159	8000.059031	11.448090	-0.059314	4.816023
290.252138	8000.029714	11.453095	-0.059287	4.816015
290.495918	8000.065149	11.458099	-0.059333	4.816024
290.637524	8000.003613	11.463104	-0.059359	4.816005
290.479672	8000.012498	11.468109	-0.059330	4.816009
290.514773	8000.028102	11.473114	-0.059336	4.816013
290.628008	7999.966050	11.478119	-0.059357	4.815995
290.460576	8000.032467	11.483123	-0.059326	4.816015
290.284315	8000.016438	11.488128	-0.059293	4.816011
290.398179	7999.984319	11.493133	-0.059315	4.816001
290.505036	8000.037565	11.498138	-0.059335	4.816016
290.432166	8000.010594	11.503143	-0.059321	4.816009
290.539829	8000.051031	11.508147	-0.059341	4.816020
290.560193	8000.040720	11.513152	-0.059345	4.816017
290.469535	8000.043347	11.518157	-0.059328	4.816018
290.373957	8000.067259	11.523162	-0.059310	4.816025
290.520836	8000.026123	11.528167	-0.059338	4.816013
290.560398	8000.062114	11.533171	-0.059345	4.816023
290.398931	8000.070933	11.538176	-0.059315	4.816026
290.601814	8000.039366	11.543181	-0.059353	4.816016
290.526725	8000.055102	11.548186	-0.059339	4.816021
290.372597	8000.003141	11.553191	-0.059310	4.816007
290.471734	8000.076551	11.558195	-0.059329	4.816028
290.551168	8000.053423	11.563200	-0.059344	4.816020
290.526058	8000.011292	11.568205	-0.059339	4.816008
290.463461	8000.050765	11.573210	-0.059328	4.816020
290.495221	8000.063103	11.578215	-0.059334	4.816024
290.562559	8000.052579	11.583219	-0.059346	4.816020
290.492631	8000.045966	11.588224	-0.059333	4.816019
290.477603	8000.027529	11.593229	-0.059330	4.816013
290.545132	8000.044794	11.598234	-0.059343	4.816018
290.506486	8000.022721	11.603239	-0.059336	4.816012
290.686837	8000.059139	11.608243	-0.059369	4.816021
290.579069	8000.025120	11.613248	-0.059349	4.816012
290.512284	7999.981162	11.618253	-0.059337	4.816000
290.461217	8000.057179	11.623258	-0.059328	4.816022
290.545819	8000.017047	11.628263	-0.059343	4.816010
290.853864	8000.089988	11.633267	-0.059401	4.816030
290.636227	8000.031526	11.638272	-0.059360	4.816014
290.599359	8000.070400	11.643277	-0.059353	4.816025
290.839842	8000.104707	11.648282	-0.059398	4.816034
290.411285	7999.963323	11.653287	-0.059318	4.815995
290.395797	8000.038920	11.658291	-0.059316	4.816017
290.514402	8000.044290	11.663296	-0.059338	4.816018
290.730104	7999.995859	11.668301	-0.059378	4.816003
290.694819	8000.076439	11.673306	-0.059372	4.816026
290.649204	8000.061720	11.678311	-0.059363	4.816022
290.811446	8000.084984	11.683315	-0.059393	4.816028
290.623509	8000.044162	11.688320	-0.059358	4.816017
290.695469	8000.060438	11.693325	-0.059372	4.816022
290.805283	8000.069924	11.698330	-0.059392	4.816024
290.644029	8000.040274	11.703335	-0.059362	4.816016
290.553252	8000.084577	11.708339	-0.059345	4.816030
290.593978	8000.042577	11.713344	-0.059353	4.816017
290.606757	8000.036402	11.718349	-0.059356	4.816015
290.419280	8000.066120	11.723354	-0.059321	4.816025
290.555182	8000.024785	11.728359	-0.059346	4.816012
290.774809	8000.014897	11.733363	-0.059387	4.816008
290.477718	8000.014833	11.738368	-0.059332	4.816010
290.498655	8000.065446	11.743373	-0.059336	4.816024
290.508630	8000.096623	11.748378	-0.059338	4.816033
290.617273	8000.029143	11.753383	-0.059358	4.816013
290.806355	8000.123429	11.758387	-0.059393	4.816040
290.618253	8000.092221	11.763392	-0.059358	4.816031
290.734564	8000.056941	11.768397	-0.059380	4.816020
290.794249	8000.077268	11.773402	-0.059391	4.816026
290.595508	8000.024494	11.778407	-0.059354	4.816012
290.784354	8000.036487	11.783411	-0.059389	4.816014
290.745233	8000.067839	11.788416	-0.059382	4.816024
290.789630	8000.017356	11.793421	-0.059390	4.816009
290.738889	8000.075213	11.798426	-0.059381	4.816026
290.647857	8000.035087	11.803431	-0.059364	4.816015
290.608706	8000.052545	11.808435	-0.059357	4.816020
290.630350	8000.080729	11.813440	-0.059361	4.816028
290.737519	8000.030321	11.818445	-0.059381	4.816013
290.512862	8000.046538	11.823450	-0.059339	4.816019
290.535804	8000.033068	11.828455	-0.059343	4.816015
290.671688	8000.079362	11.833459	-0.059369	4.816027
290.590790	8000.033009	11.838464	-0.059354	4.816014
290.523014	8000.055290	11.843469	-0.059341	4.816021
290.704229	8000.069281	11.848474	-0.059375	4.816024
290.797925	8000.035726	11.853479	-0.059392	4.816014
290.765499	8000.055445	11.858483	-0.059386	4.816020
290.715772	8000.063093	11.863488	-0.059377	4.816022
290.761831	8000.076760	11.868493	-0.059386	4.816026
290.893954	8000.059935	11.873498	-0.059410	4.816020
290.847797	8000.087953	11.878503	-0.059402	4.816029
290.895274	8000.137981	11.883507	-0.059411	4.816043
290.682484	8000.087087	11.888512	-0.059371	4.816030
290.570588	7999.997423	11.893517	-0.059350	4.816004
290.483033	8000.004382	11.898522	-0.059334	4.816006
290.757498	8000.015797	11.903527	-0.059385	4.816008
290.719013	8000.074946	11.908531	-0.059378	4.816026
290.593869	8000.065190	11.913536	-0.059355	4.816024
290.548251	8000.051540	11.918541	-0.059346	4.816020
290.703805	8000.069339	11.923546	-0.059375	4.816024
290.671873	8000.067693	11.928551	-0.059370	4.816024
290.893386	8000.132647	11.933555	-0.059411	4.816042
290.768505	8000.115414	11.938560	-0.059388	4.816037
290.772136	8000.065257	11.943565	-0.059388	4.816023
290.761641	8000.114229	11.948570	-0.059386	4.816037
290.644749	8000.119585	11.953575	-0.059365	4.816039
290.814389	8000.132298	11.958579	-0.059396	4.816042
290.639659	8000.098128	11.963584	-0.059364	4.816033
290.826222	8000.073745	11.968589	-0.059399	4.816025
290.689133	8000.116136	11.973594	-0.059373	4.816038
290.715223	8000.101654	11.978599	-0.059378	4.816034
290.775757	8000.118792	11.983603	-0.059389	4.816038
290.740304	8000.082884	11.988608	-0.059383	4.816028
290.629606	8000.070185	11.993613	-0.059362	4.816025
290.622893	8000.071136	11.998618	-0.059361	4.816025
290.915444	8000.004868	12.003623	-0.059416	4.816004
290.794331	8000.086023	12.008627	-0.059393	4.816029
290.884543	8000.074846	12.013632	-0.059410	4.816025
290.962038	8000.096567	12.018637	-0.059424	4.816031
290.902839	8000.093356	12.023642	-0.059413	4.816030
290.694970	8000.051101	12.028647	-0.059375	4.816019
290.848354	8000.052831	12.033651	-0.059403	4.816019
290.757460	8000.055454	12.038656	-0.059386	4.816020
290.866575	8000.092713	12.043661	-0.059407	4.816030
290.672104	8000.084900	12.048666	-0.059371	4.816029
290.725169	8000.058085	12.053671	-0.059381	4.816021
290.738901	8000.063683	12.058675	-0.059383	4.816022
290.528383	8000.044891	12.063680	-0.059344	4.816018
290.698266	8000.018067	12.068685	-0.059376	4.816009
290.591505	8000.085590	12.073690	-0.059356	4.816030
290.659689	8000.050502	12.078695	-0.059369	4.816019
290.775484	8000.087882	12.083699	-0.059390	4.816029
290.783524	8000.028187	12.088704	-0.059392	4.816012
290.788664	8000.033628	12.093709	-0.059393	4.816013
290.690593	8000.058563	12.098714	-0.059375	4.816021
290.755008	8000.044779	12.103719	-0.059387	4.816017
290.887456	8000.077119	12.108723	-0.059411	4.816025
290.642568	8000.027779	12.113728	-0.059366	4.816012
290.728113	7999.987663	12.118733	-0.059382	4.816000
291.002169	8000.085634	12.123738	-0.059433	4.816027
290.967831	8000.082875	12.128743	-0.059426	4.816027
291.045895	8000.099263	12.133747	-0.059441	4.816031
291.075716	8000.066682	12.138752	-0.059447	4.816021
290.873341	8000.011703	12.143757	-0.059409	4.816006
290.758578	8000.059845	12.148762	-0.059388	4.816021
290.818316	8000.005366	12.153767	-0.059399	4.816005
290.789359	8000.104230	12.158771	-0.059393	4.816034
290.756252	8000.064090	12.163776	-0.059387	4.816022
290.872222	8000.021323	12.168781	-0.059409	4.816009
290.940949	8000.070669	12.173786	-0.059422	4.816023
290.880133	8000.020407	12.178791	-0.059410	4.816009
290.899371	8000.039998	12.183795	-0.059414	4.816015
291.024806	8000.085034	12.188800	-0.059438	4.816027
290.888600	8000.047291	12.193805	-0.059412	4.816017
290.832006	8000.108247	12.198810	-0.059402	4.816035
290.851187	8000.039137	12.203815	-0.059405	4.816015
291.079122	8000.110621	12.208819	-0.059448	4.816034
290.914268	8000.076630	12.213824	-0.059417	4.816025
290.767812	8000.130606	12.218829	-0.059390	4.816042
291.044559	8000.111073	12.223834	-0.059442	4.816035
290.849178	8000.063702	12.228839	-0.059405	4.816022
290.735397	8000.078732	12.233843	-0.059384	4.816027
290.839552	8000.088115	12.238848	-0.059404	4.816029
290.827893	8000.020580	12.243853	-0.059401	4.816009
290.797005	8000.072387	12.248858	-0.059396	4.816025
290.960062	8000.042233	12.253863	-0.059426	4.816015
291.087750	8000.042426	12.258867	-0.059450	4.816014
290.962969	8000.041226	12.263872	-0.059427	4.816015
290.802382	7999.993421	12.268877	-0.059397	4.816001
290.834003	8000.045297	12.273882	-0.059403	4.816016
290.908931	7999.999645	12.278887	-0.059417	4.816003
290.935181	8000.043943	12.283891	-0.059422	4.816015
290.990746	8000.051371	12.288896	-0.059432	4.816017
290.965449	8000.017786	12.293901	-0.059427	4.816008
291.003043	8000.039849	12.298906	-0.059434	4.816014
290.869255	8000.000012	12.303911	-0.059410	4.816003
291.093605	8000.077842	12.308915	-0.059451	4.816025
291.170157	8000.047181	12.313920	-0.059466	4.816015
290.885243	8000.040926	12.318925	-0.059413	4.816015
290.837320	8000.087079	12.323930	-0.059404	4.816029
290.924590	8000.025621	12.328935	-0.059420	4.816010
291.018421	8000.140615	12.333939	-0.059438	4.816043
291.018060	8000.056187	12.338944	-0.059438	4.816019
291.034955	8000.041538	12.343949	-0.059441	4.816014
291.184247	8000.104108	12.348954	-0.059469	4.816032
290.902332	8000.057298	12.353959	-0.059416	4.816020
291.056422	8000.081483	12.358963	-0.059445	4.816026
291.133303	8000.068995	12.363968	-0.059459	4.816022
291.152163	8000.084304	12.368973	-0.059463	4.816026
291.227989	8000.081415	12.373978	-0.059477	4.816025
291.073299	8000.032648	12.378983	-0.059448	4.816011
291.020339	8000.080847	12.383987	-0.059438	4.816026
290.931171	8000.084570	12.388992	-0.059422	4.816027
291.070954	8000.049717	12.393997	-0.059448	4.816016
291.137765	8000.047733	12.399002	-0.059460	4.816015
290.952055	8000.059315	12.404007	-0.059426	4.816020
291.039853	8000.071606	12.409011	-0.059442	4.816023
290.874875	8000.050437	12.414016	-0.059412	4.816018
290.877668	8000.022707	12.419021	-0.059412	4.816010
291.125375	8000.044323	12.424026	-0.059458	4.816015
290.926446	7999.992613	12.429031	-0.059421	4.816000
290.911572	8000.094939	12.434035	-0.059419	4.816030
290.924695	8000.102663	12.439040	-0.059421	4.816033
290.999686	8000.053806	12.444045	-0.059435	4.816018
291.214452	8000.115432	12.449050	-0.059475	4.816035
291.027967	8000.071429	12.454055	-0.059440	4.816023
291.052425	8000.118900	12.459059	-0.059445	4.816037
290.877010	8000.055863	12.464064	-0.059412	4.816019
290.773142	8000.045426	12.469069	-0.059393	4.816017
291.016035	8000.057336	12.474074	-0.059438	4.816019
291.082427	7999.995498	12.479079	-0.059451	4.816000
290.930986	8000.111366	12.484083	-0.059423	4.816035
290.934149	8000.090055	12.489088	-0.059423	4.816029
291.137527	8000.007201	12.494093	-0.059461	4.816004
291.121908	8000.112720	12.499098	-0.059458	4.816035
291.021760	8000.057466	12.504103	-0.059440	4.816019
291.191931	8000.105455	12.509107	-0.059472	4.816032
291.110637	8000.067643	12.514112	-0.059456	4.816021
291.217708	8000.059980	12.519117	-0.059476	4.816019
291.255736	8000.100219	12.524122	-0.059484	4.816030
291.185493	8000.041234	12.529127	-0.059470	4.816013
291.062906	8000.094577	12.534131	-0.059448	4.816030
291.023355	8000.076762	12.539136	-0.059440	4.816025
291.277280	8000.087804	12.544141	-0.059488	4.816026
291.303673	8000.091496	12.549146	-0.059493	4.816027
291.070940	8000.034894	12.554151	-0.059449	4.816012
291.248372	8000.096909	12.559155	-0.059482	4.816029
291.045383	8000.067566	12.564160	-0.059445	4.816022
290.929360	8000.049427	12.569165	-0.059423	4.816017
291.130144	8000.078737	12.574170	-0.059461	4.816025
291.094480	8000.050306	12.579175	-0.059454	4.816016
291.185703	8000.057316	12.584179	-0.059471	4.816018
291.215262	8000.047172	12.589184	-0.059477	4.816015
291.147676	8000.082280	12.594189	-0.059464	4.816025
291.091407	8000.072710	12.599194	-0.059454	4.816023
291.088838	8000.042745	12.604199	-0.059453	4.816014
291.192365	8000.037154	12.609203	-0.059472	4.816012
291.154947	8000.068537	12.614208	-0.059466	4.816021
291.088221	7999.992519	12.619213	-0.059453	4.816000
291.161110	8000.072933	12.624218	-0.059467	4.816023
291.084486	8000.040550	12.629223	-0.059453	4.816014
291.250638	8000.061749	12.634227	-0.059484	4.816019
291.136763	8000.036167	12.639232	-0.059462	4.816012
291.087186	7999.986109	12.644237	-0.059453	4.815998
291.219080	8000.064393	12.649242	-0.059478	4.816020
291.013314	7999.990116	12.654247	-0.059439	4.815999
291.178583	7999.994199	12.659251	-0.059470	4.816000
291.141333	8000.029860	12.664256	-0.059463	4.816010
291.058337	8000.021940	12.669261	-0.059448	4.816008
291.206215	8000.091966	12.674266	-0.059476	4.816028
291.235616	8000.036934	12.679271	-0.059481	4.816012
291.217311	8000.101795	12.684275	-0.059478	4.816031
291.222911	8000.073046	12.689280	-0.059479	4.816022
291.149161	8000.027891	12.694285	-0.059465	4.816010
291.311762	8000.045820	12.699290	-0.059495	4.816014
291.083119	8000.025628	12.704295	-0.059453	4.816009
291.064023	8000.046658	12.709299	-0.059449	4.816015
291.061690	8000.046620	12.714304	-0.059449	4.816015
291.153855	8000.031205	12.719309	-0.059466	4.816010
291.039523	8000.076148	12.724314	-0.059445	4.816024
291.110185	8000.044310	12.729319	-0.059458	4.816015
291.131032	8000.045763	12.734323	-0.059462	4.816015
291.072996	8000.054328	12.739328	-0.059451	4.816018
291.127584	8000.004031	12.744333	-0.059462	4.816003
291.164471	8000.056004	12.749338	-0.059469	4.816018
290.883596	8000.026312	12.754343	-0.059416	4.816010
291.269819	8000.038695	12.759347	-0.059488	4.816012
291.272387	8000.045159	12.764352	-0.059489	4.816014
291.255088	8000.054466	12.769357	-0.059486	4.816017
291.300672	8000.084155	12.774362	-0.059494	4.816025
291.240066	8000.003973	12.779367	-0.059483	4.816002
291.216393	8000.030263	12.784371	-0.059478	4.816010
291.119089	8000.015670	12.789376	-0.059460	4.816006
291.037922	8000.038776	12.794381	-0.059445	4.816013
291.075075	8000.104646	12.799386	-0.059452	4.816032
290.919771	8000.006709	12.804391	-0.059423	4.816005
291.042448	8000.016429	12.809395	-0.059446	4.816007
291.287306	8000.073259	12.814400	-0.059492	4.816022
291.395216	8000.058131	12.819405	-0.059512	4.816017
291.389447	8000.126426	12.824410	-0.059511	4.816037
291.354176	8000.060598	12.829415	-0.059505	4.816018
291.542614	8000.039456	12.834419	-0.059540	4.816011
291.283535	8000.070006	12.839424	-0.059491	4.816021
291.184865	8000.041496	12.844429	-0.059473	4.816013
291.432070	8000.064172	12.849434	-0.059519	4.816019
291.335817	8000.033568	12.854439	-0.059501	4.816010
291.369066	8000.009598	12.859443	-0.059508	4.816003
291.372069	8000.034237	12.864448	-0.059508	4.816010
291.313544	8000.040656	12.869453	-0.059497	4.816012
291.475130	8000.056429	12.874458	-0.059527	4.816016
291.218393	8000.001527	12.879463	-0.059480	4.816001
291.260676	8000.016195	12.884467	-0.059488	4.816005
291.180977	8000.031846	12.889472	-0.059473	4.816010
291.223016	8000.026204	12.894477	-0.059481	4.816009
291.151400	8000.060170	12.899482	-0.059467	4.816019
291.094076	7999.947988	12.904487	-0.059457	4.815986
291.168716	8000.014541	12.909491	-0.059471	4.816005
291.153781	8000.014273	12.914496	-0.059468	4.816005
291.289115	7999.985752	12.919501	-0.059493	4.815996
291.135099	8000.058826	12.924506	-0.059465	4.816019
291.219963	8000.041140	12.929511	-0.059480	4.816013
291.341921	8000.054054	12.934515	-0.059503	4.816016
291.375601	8000.064290	12.939520	-0.059510	4.816019
291.216611	7999.994070	12.944525	-0.059480	4.815999
291.130108	8000.067306	12.949530	-0.059464	4.816021
291.266583	8000.042011	12.954535	-0.059489	4.816013
291.362539	8000.058726	12.959539	-0.059507	4.816017
291.337852	8000.045456	12.964544	-0.059503	4.816014
291.300557	8000.041575	12.969549	-0.059496	4.816013
291.127672	8000.071558	12.974554	-0.059464	4.816022
291.048979	8000.039137	12.979559	-0.059449	4.816013
291.285503	8000.044519	12.984563	-0.059493	4.816014
291.175838	8000.066037	12.989568	-0.059473	4.816020
291.167569	8000.047723	12.994573	-0.059471	4.816015
291.291803	8000.106631	12.999578	-0.059494	4.816032
291.305041	7999.998939	13.004583	-0.059497	4.816000
291.228975	8000.001833	13.009587	-0.059483	4.816001
291.281688	8000.060506	13.014592	-0.059493	4.816018
291.528208	8000.039354	13.019597	-0.059539	4.816011
291.584611	8000.121606	13.024602	-0.059549	4.816035
291.452481	8000.079661	13.029607	-0.059525	4.816023
291.444721	8000.073112	13.034611	-0.059523	4.816021
291.217036	8000.056144	13.039616	-0.059481	4.816017
291.230341	7999.974102	13.044621	-0.059483	4.815993
291.393840	8000.072198	13.049626	-0.059514	4.816021
291.249128	8000.069566	13.054631	-0.059487	4.816021
291.457981	8000.069101	13.059635	-0.059526	4.816020
291.480306	8000.097298	13.064640	-0.059530	4.816028
291.458036	8000.052011	13.069645	-0.059526	4.816015
291.287064	8000.089511	13.074650	-0.059494	4.816027
291.387151	8000.018668	13.079655	-0.059513	4.816005
291.582461	8000.085284	13.084659	-0.059549	4.816024
291.544668	8000.118797	13.089664	-0.059542	4.816034
291.663131	8000.075007	13.094669	-0.059564	4.816020
291.590856	8000.117510	13.099674	-0.059551	4.816033
291.303866	8000.008623	13.104679	-0.059498	4.816003
291.361567	8000.079143	13.109683	-0.059508	4.816023
291.367269	8000.081389	13.114688	-0.059510	4.816024
291.452772	8000.045547	13.119693	-0.059525	4.816013
291.438643	8000.069873	13.124698	-0.059523	4.816020
291.368325	8000.069665	13.129703	-0.059510	4.816020
291.538882	8000.067434	13.134707	-0.059542	4.816019
291.529434	8000.064060	13.139712	-0.059540	4.816018
291.281484	8000.028555	13.144717	-0.059494	4.816009
291.550956	8000.081560	13.149722	-0.059544	4.816023
291.519952	8000.046801	13.154727	-0.059538	4.816013
291.502346	8000.098850	13.159731	-0.059535	4.816028
291.412999	8000.101501	13.164736	-0.059518	4.816030
291.373664	8000.044149	13.169741	-0.059511	4.816013
291.604039	8000.144533	13.174746	-0.059554	4.816041
291.298790	8000.080197	13.179751	-0.059497	4.816024
291.364347	8000.129487	13.184755	-0.059510	4.816038
291.474300	8000.136838	13.189760	-0.059530	4.816040
291.571614	8000.072357	13.194765	-0.059548	4.816020
291.574037	8000.113016	13.199770	-0.059549	4.816032
291.548692	8000.018514	13.204775	-0.059544	4.816005
291.524147	8000.091810	13.209779	-0.059540	4.816026
291.309894	8000.099666	13.214784	-0.059500	4.816030
291.371181	8000.089032	13.219789	-0.059511	4.816026
291.538283	8000.085669	13.224794	-0.059542	4.816024
291.383410	8000.044378	13.229799	-0.059514	4.816013
291.427393	8000.090069	13.234803	-0.059522	4.816026
291.469687	8000.094050	13.239808	-0.059530	4.816027
291.623695	8000.081899	13.244813	-0.059558	4.816023
291.648838	8000.135796	13.249818	-0.059563	4.816038
291.449640	8000.086217	13.254823	-0.059526	4.816025
291.546966	8000.115781	13.259827	-0.059544	4.816033
291.577210	8000.104581	13.264832	-0.059550	4.816030
291.533605	8000.039669	13.269837	-0.059542	4.816011
291.683070	8000.090488	13.274842	-0.059570	4.816025
291.400238	8000.036179	13.279847	-0.059517	4.816010
291.394955	8000.055323	13.284851	-0.059516	4.816016
291.390182	8000.086232	13.289856	-0.059515	4.816025
291.331746	8000.052043	13.294861	-0.059504	4.816015
291.408055	8000.083361	13.299866	-0.059519	4.816024
291.553654	8000.063576	13.304871	-0.059546	4.816018
291.711247	8000.052559	13.309875	-0.059575	4.816014
291.347029	8000.091880	13.314880	-0.059508	4.816027
291.481435	8000.036624	13.319885	-0.059533	4.816010
291.532265	8000.086714	13.324890	-0.059542	4.816025
291.468138	8000.077001	13.329895	-0.059530	4.816022
291.616813	8000.083989	13.334899	-0.059558	4.816023
291.743382	8000.104468	13.339904	-0.059582	4.816029
291.550250	8000.073166	13.344909	-0.059546	4.816020
291.511964	8000.105603	13.349914	-0.059539	4.816030
291.351309	8000.077031	13.354919	-0.059509	4.816023
291.558979	8000.100056	13.359923	-0.059547	4.816028
291.489447	8000.084900	13.364928	-0.059534	4.816024
291.427490	8000.083776	13.369933	-0.059523	4.816024
291.565009	8000.126896	13.374938	-0.059549	4.816036
291.249075	8000.098701	13.379943	-0.059490	4.816030
291.329602	8000.092692	13.384947	-0.059505	4.816027
291.476642	8000.117818	13.389952	-0.059532	4.816034
291.340810	8000.107866	13.394957	-0.059507	4.816032
291.394728	8000.091754	13.399962	-0.059517	4.816027
291.317745	8000.072188	13.404967	-0.059503	4.816021
291.549430	8000.135192	13.409971	-0.059546	4.816039
291.554757	8000.117126	13.414976	-0.059547	4.816033
291.364986	8000.068787	13.419981	-0.059512	4.816020
291.658701	8000.133990	13.424986	-0.059567	4.816038
291.527783	8000.052526	13.429991	-0.059542	4.816015
291.503609	8000.079875	13.434995	-0.059538	4.816023
291.531574	8000.083595	13.440000	-0.059543	4.816024
291.454239	8000.074710	13.445005	-0.059529	4.816021
291.697735	8000.109075	13.450010	-0.059574	4.816030
291.530748	8000.070769	13.455015	-0.059543	4.816020
291.494011	8000.087203	13.460019	-0.059536	4.816025
291.685989	8000.080019	13.465024	-0.059572	4.816022
291.729709	8000.073339	13.470029	-0.059580	4.816020
291.696632	8000.106939	13.475034	-0.059574	4.816030
291.654453	8000.091213	13.480039	-0.059566	4.816025
291.540978	8000.026097	13.485043	-0.059545	4.816007
291.599698	8000.082743	13.490048	-0.059556	4.816023
291.662748	8000.047560	13.495053	-0.059568	4.816012
291.685817	8000.117450	13.500058	-0.059572	4.816033
291.644922	8000.109229	13.505063	-0.059565	4.816030
291.695603	8000.089851	13.510067	-0.059574	4.816025
291.481806	8000.109471	13.515072	-0.059534	4.816031
291.500771	8000.102340	13.520077	-0.059538	4.816029
291.634020	8000.100498	13.525082	-0.059563	4.816028
291.485584	8000.053981	13.530087	-0.059535	4.816015
291.427200	8000.049715	13.535091	-0.059524	4.816014
291.676086	8000.116239	13.540096	-0.059571	4.816032
291.658154	8000.096680	13.545101	-0.059567	4.816027
291.528111	8000.116757	13.550106	-0.059543	4.816033
291.440219	8000.085237	13.555111	-0.059527	4.816025
291.667720	8000.093661	13.560115	-0.059569	4.816026
291.631376	8000.087660	13.565120	-0.059563	4.816024
291.535685	8000.031417	13.570125	-0.059545	4.816008
291.717447	8000.098855	13.575130	-0.059579	4.816027
291.568386	8000.073701	13.580135	-0.059551	4.816020
291.562160	8000.077866	13.585139	-0.059550	4.816022
291.637795	8000.114516	13.590144	-0.059564	4.816032
291.553500	8000.058481	13.595149	-0.059548	4.816016
291.603462	8000.124586	13.600154	-0.059558	4.816035
291.607666	8000.075507	13.605159	-0.059559	4.816021
291.613693	8000.044629	13.610163	-0.059560	4.816012
291.564805	8000.052292	13.615168	-0.059551	4.816014
291.491893	7999.992190	13.620173	-0.059537	4.815997
291.530056	8000.136094	13.625178	-0.059544	4.816039
291.533841	8000.109450	13.630183	-0.059545	4.816031
291.516404	8000.083488	13.635187	-0.059542	4.816024
291.612932	8000.101282	13.640192	-0.059560	4.816028
291.585660	8000.055904	13.645197	-0.059555	4.816015
291.455045	8000.127268	13.650202	-0.059531	4.816037
291.509558	8000.053457	13.655207	-0.059541	4.816015
291.755475	8000.107103	13.660211	-0.059587	4.816029
291.703237	8000.068751	13.665216	-0.059577	4.816018
291.626696	8000.087666	13.670221	-0.059563	4.816024
291.634246	8000.130555	13.675226	-0.059564	4.816037
291.698549	8000.088984	13.680231	-0.059576	4.816024
291.639795	8000.100742	13.685235	-0.059565	4.816028
291.692276	8000.105977	13.690240	-0.059575	4.816029
291.743586	8000.094092	13.695245	-0.059585	4.816025
291.767019	8000.135134	13.700250	-0.059589	4.816037
291.597715	8000.077550	13.705255	-0.059558	4.816021
291.625040	8000.114387	13.710259	-0.059563	4.816032
291.852200	8000.137768	13.715264	-0.059605	4.816038
291.719643	8000.090471	13.720269	-0.059580	4.816025
291.688119	8000.136924	13.725274	-0.059575	4.816038
291.809400	8000.088910	13.730279	-0.059597	4.816024
291.923945	8000.049322	13.735283	-0.059619	4.816011
291.811914	8000.125300	13.740288	-0.059598	4.816034
291.746552	8000.086709	13.745293	-0.059586	4.816023
292.004972	8000.123484	13.750298	-0.059634	4.816033
291.641196	8000.118996	13.755303	-0.059566	4.816033
291.793711	8000.061932	13.760307	-0.059595	4.816016
291.768552	8000.093539	13.765312	-0.059590	4.816025
291.653479	8000.050836	13.770317	-0.059569	4.816013
291.751494	8000.100718	13.775322	-0.059587	4.816027
291.773138	8000.091498	13.780327	-0.059591	4.816025
291.715559	8000.126789	13.785331	-0.059580	4.816035
291.717799	8000.130040	13.790336	-0.059581	4.816036
291.700874	8000.077370	13.795341	-0.059578	4.816021
291.810292	8000.125322	13.800346	-0.059598	4.816034
291.618283	8000.042744	13.805351	-0.059562	4.816011
291.745836	8000.058966	13.810355	-0.059586	4.816015
291.927287	8000.087926	13.815360	-0.059620	4.816023
291.757441	8000.065598	13.820365	-0.059588	4.816017
291.775103	8000.108672	13.825370	-0.059592	4.816030
291.686664	8000.083554	13.830375	-0.059575	4.816023
291.727226	8000.088572	13.835379	-0.059583	4.816024
291.619264	8000.095158	13.840384	-0.059563	4.816026
291.653845	8000.042358	13.845389	-0.059569	4.816011
291.778068	8000.082031	13.850394	-0.059593	4.816022
291.864788	8000.050486	13.855399	-0.059609	4.816012
291.919866	8000.039738	13.860403	-0.059619	4.816009
291.769154	8000.044477	13.865408	-0.059591	4.816011
291.795745	7999.991531	13.870413	-0.059596	4.815995
291.857122	8000.089905	13.875418	-0.059607	4.816024
291.865088	8000.036620	13.880423	-0.059609	4.816008
291.905204	8000.019187	13.885427	-0.059616	4.816003
291.927626	8000.079447	13.890432	-0.059621	4.816020
291.764584	8000.081824	13.895437	-0.059590	4.816022
291.914666	8000.076014	13.900442	-0.059618	4.816019
291.889365	8000.043496	13.905447	-0.059614	4.816010
291.831461	8000.059544	13.910451	-0.059603	4.816015
291.925565	8000.104012	13.915456	-0.059621	4.816027
291.896410	8000.027607	13.920461	-0.059615	4.816005
292.013110	8000.075692	13.925466	-0.059637	4.816019
291.977091	8000.073971	13.930471	-0.059630	4.816018
291.874885	8000.082800	13.935475	-0.059611	4.816021
291.822681	8000.109639	13.940480	-0.059602	4.816030
291.714430	8000.086297	13.945485	-0.059582	4.816023
291.887038	8000.074485	13.950490	-0.059614	4.816019
291.705635	8000.060496	13.955495	-0.059580	4.816016
291.560485	8000.055718	13.960499	-0.059553	4.816015
291.898401	8000.067224	13.965504	-0.059616	4.816017
291.962277	8000.065186	13.970509	-0.059628	4.816016
291.849555	8000.099472	13.975514	-0.059607	4.816026
291.876880	8000.076463	13.980519	-0.059612	4.816020
292.060834	8000.116156	13.985523	-0.059646	4.816030
291.985858	8000.144718	13.990528	-0.059632	4.816039
292.004298	8000.107653	13.995533	-0.059636	4.816028
291.964559	8000.143269	14.000538	-0.059629	4.816039
291.860070	8000.093278	14.005543	-0.059609	4.816025
291.661594	8000.091802	14.010547	-0.059572	4.816025
291.913675	8000.106019	14.015552	-0.059619	4.816028
291.958436	8000.049129	14.020557	-0.059628	4.816011
291.961005	8000.070554	14.025562	-0.059628	4.816017
291.875411	8000.071136	14.030567	-0.059612	4.816018
291.907222	8000.016148	14.035571	-0.059618	4.816002
291.902842	8000.076988	14.040576	-0.059617	4.816020
291.882066	8000.031729	14.045581	-0.059614	4.816006
291.993931	8000.098962	14.050586	-0.059634	4.816025
291.742246	8000.037739	14.055591	-0.059588	4.816009
291.939992	8000.059515	14.060595	-0.059625	4.816014
292.061789	8000.148304	14.065600	-0.059647	4.816040
291.898919	8000.041676	14.070605	-0.059617	4.816009
291.833747	8000.045836	14.075610	-0.059605	4.816011
291.743097	8000.038845	14.080615	-0.059588	4.816009
291.824244	8000.049946	14.085619	-0.059603	4.816012
291.752711	8000.105288	14.090624	-0.059590	4.816029
291.537802	8000.075727	14.095629	-0.059550	4.816021
292.013341	8000.123940	14.100634	-0.059639	4.816033
291.809495	8000.070000	14.105639	-0.059601	4.816018
291.713748	8000.082153	14.110643	-0.059583	4.816022
291.852910	8000.082556	14.115648	-0.059609	4.816021
291.793048	8000.059026	14.120653	-0.059598	4.816015
291.826376	8000.132310	14.125658	-0.059604	4.816036
291.942912	8000.130163	14.130663	-0.059626	4.816035
292.056378	8000.114068	14.135667	-0.059647	4.816030
291.972173	8000.069789	14.140672	-0.059631	4.816017
292.055094	8000.098022	14.145677	-0.059647	4.816025
292.212145	8000.107301	14.150682	-0.059676	4.816027
292.098850	8000.058218	14.155687	-0.059655	4.816013
291.806224	8000.040065	14.160691	-0.059600	4.816009
291.891361	8000.086506	14.165696	-0.059616	4.816022
291.963635	8000.087827	14.170701	-0.059630	4.816022
291.943926	8000.104572	14.175706	-0.059626	4.816027
291.878518	8000.078804	14.180711	-0.059614	4.816020
291.740433	8000.106215	14.185715	-0.059588	4.816029
291.866336	8000.122407	14.190720	-0.059612	4.816033
291.620261	8000.097622	14.195725	-0.059566	4.816027
291.908194	8000.063331	14.200730	-0.059620	4.816015
291.938509	8000.091675	14.205735	-0.059626	4.816024
291.875515	7999.990073	14.210739	-0.059614	4.815994
291.989031	8000.072299	14.215744	-0.059635	4.816018
291.946066	8000.034115	14.220749	-0.059627	4.816007
291.936211	8000.057452	14.225754	-0.059625	4.816014
292.053940	8000.058533	14.230759	-0.059647	4.816013
292.157056	8000.133089	14.235763	-0.059667	4.816035
292.241205	8000.132490	14.240768	-0.059682	4.816034
291.787922	8000.056904	14.245773	-0.059598	4.816014
291.932959	8000.122605	14.250778	-0.059625	4.816033
292.063907	8000.089729	14.255783	-0.059649	4.816022
291.921911	8000.074320	14.260787	-0.059623	4.816019
291.970182	8000.077342	14.265792	-0.059632	4.816019
291.953057	7999.123779	14.270797	-0.059628	4.815741

291.797992	7995.955965	14.275802	-0.059597	4.814816
291.642992	7990.561696	14.280807	-0.059565	4.813240
291.903405	7983.906105	14.285811	-0.059609	4.811293
292.068072	7976.649539	14.290816	-0.059635	4.809170
291.802338	7969.022731	14.295821	-0.059581	4.806939
291.921000	7961.234556	14.300826	-0.059598	4.804659
291.777435	7953.381622	14.305831	-0.059566	4.802360
291.656064	7945.340097	14.310835	-0.059538	4.800004
291.519908	7937.525897	14.315840	-0.059508	4.797713
291.492857	7929.392739	14.320845	-0.059498	4.795328
291.582342	7921.445289	14.325850	-0.059509	4.792995
291.511041	7913.350267	14.330855	-0.059491	4.790619
291.470199	7905.400034	14.335859	-0.059478	4.788283
291.532865	7897.427719	14.340864	-0.059484	4.785940
291.234464	7889.433521	14.345869	-0.059424	4.783591
291.246242	7881.449188	14.350874	-0.059421	4.781242
291.162592	7873.386747	14.355879	-0.059400	4.778869
291.277683	7865.421410	14.360883	-0.059416	4.776523
291.268060	7857.376542	14.365888	-0.059409	4.774153
291.217696	7849.384854	14.370893	-0.059395	4.771797
291.287779	7841.404160	14.375898	-0.059402	4.769443
291.021183	7833.417334	14.380903	-0.059348	4.767087
290.971122	7825.354065	14.385907	-0.059333	4.764707
290.953264	7817.453806	14.390912	-0.059325	4.762374
290.836437	7809.341682	14.395917	-0.059298	4.759977
290.853292	7801.419172	14.400922	-0.059296	4.757635
290.829682	7793.373413	14.405927	-0.059286	4.755255
290.788002	7785.363105	14.410931	-0.059273	4.752884
290.683813	7777.352857	14.415936	-0.059249	4.750513
290.543647	7769.314597	14.420941	-0.059217	4.748132
290.642365	7761.341309	14.425946	-0.059231	4.745768
290.495178	7753.347914	14.430951	-0.059198	4.743398
290.490833	7745.351878	14.435955	-0.059192	4.741026
290.775485	7737.400069	14.440960	-0.059240	4.738664
290.496687	7729.328926	14.445965	-0.059183	4.736268
290.344538	7721.361116	14.450970	-0.059149	4.733901
290.511191	7713.282301	14.455975	-0.059175	4.731499
290.314561	7705.290624	14.460979	-0.059133	4.729122
290.264383	7697.350780	14.465984	-0.059119	4.726760
290.223037	7689.304960	14.470989	-0.059106	4.724364
290.357208	7681.344706	14.475994	-0.059126	4.721992
290.348086	7673.298975	14.480999	-0.059119	4.719594
290.056846	7665.369644	14.486003	-0.059060	4.717231
290.120307	7657.342242	14.491008	-0.059066	4.714835
290.192858	7649.292852	14.496013	-0.059074	4.712432
290.080432	7641.278195	14.501018	-0.059048	4.710039
289.877734	7633.313832	14.506023	-0.059005	4.707660
289.987388	7625.307346	14.511027	-0.059021	4.705266
289.857234	7617.372686	14.516032	-0.058991	4.702893
289.778076	7609.314251	14.521037	-0.058971	4.700481
289.960189	7601.339344	14.526042	-0.059000	4.698093
289.761698	7593.288178	14.531047	-0.058958	4.695682
289.722958	7585.298757	14.536051	-0.058946	4.693287
289.769950	7577.246463	14.541056	-0.058949	4.690872
289.687859	7569.277412	14.546061	-0.058929	4.688481
289.553653	7561.309996	14.551066	-0.058899	4.686090
289.606928	7553.318980	14.556071	-0.058903	4.683690
289.548961	7545.313599	14.561075	-0.058887	4.681284
289.461185	7537.329807	14.566080	-0.058866	4.678884
289.256155	7529.350402	14.571085	-0.058823	4.676484
289.401367	7521.274800	14.576090	-0.058844	4.674053
289.353509	7513.135792	14.581095	-0.058830	4.671603
289.165262	7505.174264	14.586099	-0.058790	4.669204
289.246402	7497.230933	14.591104	-0.058800	4.666810
289.294622	7489.224198	14.596109	-0.058804	4.664395
289.169226	7481.307522	14.601114	-0.058775	4.662006
289.037760	7473.246057	14.606119	-0.058746	4.659573
289.165953	7465.257366	14.611123	-0.058764	4.657159
289.177212	7457.249475	14.616128	-0.058761	4.654739
288.939912	7449.238373	14.621133	-0.058712	4.652317
288.921116	7441.224290	14.626138	-0.058703	4.649892
288.777198	7433.225197	14.631143	-0.058671	4.647471
288.751041	7425.188576	14.636147	-0.058661	4.645037
288.868791	7417.279335	14.641152	-0.058678	4.642641
288.669595	7409.205129	14.646157	-0.058636	4.640193
288.551612	7401.273442	14.651162	-0.058609	4.637787
288.533842	7393.220798	14.656167	-0.058600	4.635343
288.696658	7385.190469	14.661171	-0.058625	4.632905
288.782550	7377.191821	14.666176	-0.058636	4.630475
288.379130	7369.202129	14.671181	-0.058556	4.628046
288.364203	7361.175738	14.676186	-0.058548	4.625605
288.293071	7353.264239	14.681191	-0.058529	4.623198
288.269695	7345.211428	14.686195	-0.058520	4.620746
288.414742	7337.227803	14.691200	-0.058542	4.618314
288.397489	7329.177376	14.696205	-0.058533	4.615860
288.230214	7321.182174	14.701210	-0.058497	4.613422
288.120845	7313.169873	14.706215	-0.058471	4.610978
288.307805	7305.149974	14.711219	-0.058501	4.608530
288.352096	7297.217919	14.716224	-0.058504	4.606107
288.074471	7289.216211	14.721229	-0.058447	4.603662
288.156459	7281.165008	14.726234	-0.058457	4.601200
288.137993	7273.191502	14.731239	-0.058449	4.598761
288.006382	7265.186520	14.736243	-0.058419	4.596311
287.876611	7257.179752	14.741248	-0.058390	4.593859
287.662922	7249.084634	14.746253	-0.058345	4.591378
287.817598	7241.111963	14.751258	-0.058368	4.588934
287.755122	7233.115107	14.756263	-0.058352	4.586481
287.733969	7225.145924	14.761267	-0.058343	4.584035
287.869145	7217.160542	14.766272	-0.058363	4.581583
287.585133	7209.142260	14.771277	-0.058304	4.579120
287.588991	7201.145303	14.776282	-0.058300	4.576661
287.651391	7193.144444	14.781287	-0.058306	4.574201
287.443521	7185.100659	14.786291	-0.058263	4.571725
287.654550	7177.120343	14.791296	-0.058297	4.569268
287.516759	7169.114573	14.796301	-0.058266	4.566802
287.704174	7161.092201	14.801306	-0.058296	4.564329
287.539035	7153.175173	14.806311	-0.058260	4.561888
287.121627	7145.132642	14.811315	-0.058177	4.559406
287.348861	7137.185831	14.816320	-0.058214	4.556952
287.241107	7129.078534	14.821325	-0.058189	4.554448
287.152316	7121.115044	14.826330	-0.058167	4.551986
287.326094	7113.111602	14.831335	-0.058194	4.549512
287.030149	7105.119206	14.836339	-0.058134	4.547038
287.075554	7097.115861	14.841344	-0.058137	4.544561
287.132174	7089.157132	14.846349	-0.058143	4.542096
287.074806	7081.100467	14.851354	-0.058127	4.539599
286.785514	7073.161015	14.856359	-0.058068	4.537136
286.778210	7065.089893	14.861363	-0.058061	4.534632
286.826105	7057.138600	14.866368	-0.058065	4.532164
286.723476	7049.056722	14.871373	-0.058041	4.529654
286.946311	7041.124313	14.876378	-0.058077	4.527189
286.744011	7033.091033	14.881383	-0.058034	4.524690
286.753740	7025.205555	14.886387	-0.058031	4.522237
286.823076	7017.161585	14.891392	-0.058039	4.519733
286.693372	7009.143285	14.896397	-0.058009	4.517236
286.811966	7001.052830	14.901402	-0.058026	4.514715
286.593287	6993.006041	14.906407	-0.057980	4.512205
286.517262	6985.047923	14.911411	-0.057961	4.509722
286.683170	6977.099589	14.916416	-0.057987	4.507242
286.376388	6969.029950	14.921421	-0.057924	4.504721
286.435852	6961.119143	14.926426	-0.057930	4.502249
286.243129	6953.081757	14.931431	-0.057889	4.499735
286.143052	6945.124068	14.936435	-0.057865	4.497245
286.221071	6937.061771	14.941440	-0.057875	4.494722
286.246935	6929.050233	14.946445	-0.057874	4.492213
286.246766	6921.051348	14.951450	-0.057869	4.489706
286.001885	6913.087843	14.956455	-0.057818	4.487208
286.065381	6905.020795	14.961459	-0.057825	4.484678
286.113461	6897.106568	14.966464	-0.057829	4.482193
286.079041	6889.020567	14.971469	-0.057817	4.479654
285.784773	6881.110378	14.976474	-0.057757	4.477167
285.856771	6873.054396	14.981479	-0.057765	4.474634
285.812582	6865.019930	14.986483	-0.057752	4.472106
285.779905	6857.057343	14.991488	-0.057741	4.469600
285.660721	6849.019834	14.996493	-0.057713	4.467068
285.599175	6840.989328	15.001498	-0.057697	4.464537
285.723556	6833.079283	15.006503	-0.057715	4.462043
285.517668	6825.045509	15.011507	-0.057671	4.459507
285.658344	6817.090802	15.016512	-0.057692	4.456997
285.354615	6809.002081	15.021517	-0.057631	4.454441
285.319395	6801.009966	15.026522	-0.057619	4.451915
285.627138	6792.980056	15.031527	-0.057671	4.449377
285.334975	6784.999955	15.036531	-0.057611	4.446850
285.281423	6777.043422	15.041536	-0.057596	4.444331
285.342379	6769.050662	15.046541	-0.057603	4.441800
285.433809	6761.026625	15.051546	-0.057614	4.439257
285.041266	6753.050476	15.056551	-0.057536	4.436726
285.062836	6744.993242	15.061555	-0.057535	4.434169
285.220467	6736.977275	15.066560	-0.057559	4.431625
285.323674	6728.956729	15.071565	-0.057573	4.429077
285.051795	6720.967249	15.076570	-0.057517	4.426537
284.975568	6712.999514	15.081575	-0.057498	4.424002
284.763203	6704.990151	15.086579	-0.057453	4.421452
284.765440	6697.014929	15.091584	-0.057449	4.418913
284.695682	6688.972799	15.096589	-0.057430	4.416350
284.981635	6681.023407	15.101594	-0.057478	4.413818
284.600819	6672.952899	15.106599	-0.057402	4.411242
284.683128	6664.982308	15.111603	-0.057413	4.408698
284.629984	6656.998719	15.116608	-0.057397	4.406148
284.687477	6648.984936	15.121613	-0.057403	4.403588
284.461373	6640.993711	15.126618	-0.057356	4.401032
284.681232	6632.990708	15.131623	-0.057391	4.398473
284.492305	6624.983935	15.136627	-0.057351	4.395909
284.407932	6616.978342	15.141632	-0.057330	4.393345
284.291236	6608.918564	15.146637	-0.057303	4.390761
284.232786	6600.976538	15.151642	-0.057287	4.388214
284.213285	6592.969458	15.156647	-0.057278	4.385645
284.058621	6585.001377	15.161651	-0.057245	4.383086
284.144223	6576.988380	15.166656	-0.057255	4.380513
283.922940	6569.019185	15.171661	-0.057209	4.377950
283.987786	6561.008180	15.176666	-0.057216	4.375374
284.050497	6553.015491	15.181671	-0.057222	4.372803
284.122779	6544.938140	15.186675	-0.057231	4.370203
284.068190	6537.008269	15.191680	-0.057215	4.367647
283.920148	6528.982093	15.196685	-0.057183	4.365059
283.911184	6521.025990	15.201690	-0.057176	4.362493
283.820431	6512.979353	15.206695	-0.057154	4.359896
283.728197	6505.026500	15.211699	-0.057131	4.357327
283.808625	6497.001781	15.216704	-0.057141	4.354734
283.748992	6488.888866	15.221709	-0.057125	4.352111
283.662090	6480.872076	15.226714	-0.057103	4.349517
283.521008	6472.945990	15.231719	-0.057072	4.346950
283.422736	6464.921685	15.236723	-0.057049	4.344350
283.685619	6456.961650	15.241728	-0.057092	4.341772
283.561334	6448.944560	15.246733	-0.057064	4.339172
283.671605	6440.994046	15.251738	-0.057079	4.336593
283.516426	6432.978567	15.256743	-0.057045	4.333989
283.254131	6424.923068	15.261747	-0.056991	4.331370
283.254830	6416.967993	15.266752	-0.056986	4.328784
283.106093	6408.938241	15.271757	-0.056953	4.326172
283.110434	6400.945701	15.276762	-0.056949	4.323570
283.051350	6392.960270	15.281767	-0.056933	4.320969
283.046601	6384.952665	15.286771	-0.056927	4.318360
283.055584	6376.973546	15.291776	-0.056923	4.315759
282.920239	6368.927743	15.296781	-0.056893	4.313133
282.917080	6360.914615	15.301786	-0.056887	4.310517
282.896130	6352.924906	15.306791	-0.056878	4.307907
282.808170	6344.910985	15.311795	-0.056857	4.305287
282.925279	6336.960380	15.316800	-0.056873	4.302687
282.864105	6328.906026	15.321805	-0.056857	4.300051
282.920353	6320.963580	15.326810	-0.056862	4.297451
282.631179	6312.900505	15.331815	-0.056803	4.294807
282.618191	6304.903710	15.336819	-0.056795	4.292185
282.577306	6296.921029	15.341824	-0.056783	4.289566
282.491949	6288.919575	15.346829	-0.056762	4.286939
282.510960	6280.919638	15.351834	-0.056760	4.284311
282.655156	6272.939654	15.356839	-0.056782	4.281690
282.303105	6264.959407	15.361843	-0.056711	4.279063
282.298618	6256.981441	15.366848	-0.056705	4.276437
282.412960	6248.870870	15.371853	-0.056721	4.273768
282.228880	6240.886383	15.376858	-0.056681	4.271135
282.108068	6232.894910	15.381863	-0.056654	4.268500
282.126958	6224.869913	15.386867	-0.056652	4.265853
282.178330	6216.905806	15.391872	-0.056657	4.263224
281.958585	6208.893986	15.396877	-0.056610	4.260576
282.073956	6200.893736	15.401882	-0.056627	4.257933
282.134091	6192.888520	15.406887	-0.056633	4.255286
281.944323	6184.897622	15.411891	-0.056592	4.252640
281.711644	6176.891231	15.416896	-0.056544	4.249987
281.639320	6168.930909	15.421901	-0.056525	4.247349
281.630708	6160.904206	15.426906	-0.056518	4.244688
281.632550	6152.936833	15.431911	-0.056514	4.242045
281.632588	6144.916189	15.436915	-0.056508	4.239382
281.622199	6136.955373	15.441920	-0.056501	4.236738
281.525037	6128.898630	15.446925	-0.056478	4.234059
281.561608	6120.896824	15.451930	-0.056480	4.231399
281.801196	6112.863439	15.456935	-0.056519	4.228727
281.538341	6104.885690	15.461939	-0.056465	4.226068
281.284195	6096.956853	15.466944	-0.056413	4.223424
281.544796	6088.922972	15.471949	-0.056456	4.220748
281.598074	6080.975799	15.476954	-0.056461	4.218097
281.268344	6072.920313	15.481959	-0.056394	4.215405
281.341984	6064.934082	15.486963	-0.056403	4.212737
281.438269	6056.899938	15.491968	-0.056415	4.210053
281.284308	6048.955697	15.496973	-0.056382	4.207394
281.126388	6040.915022	15.501978	-0.056347	4.204701
281.176645	6032.977737	15.506983	-0.056351	4.202044
280.937579	6024.939593	15.511987	-0.056302	4.199347
280.927969	6016.965866	15.516992	-0.056295	4.196673
280.925249	6008.872389	15.521997	-0.056289	4.193958
280.985499	6000.797109	15.527002	-0.056295	4.191247
281.037657	5992.870336	15.532007	-0.056299	4.188584
280.899755	5984.836584	15.537011	-0.056269	4.185882
281.044354	5976.913384	15.542016	-0.056290	4.183218
280.857085	5968.904536	15.547021	-0.056250	4.180520
280.759024	5960.917584	15.552026	-0.056227	4.177828
280.833832	5952.897002	15.557031	-0.056236	4.175125
280.769320	5944.905475	15.562035	-0.056218	4.172429
280.760045	5936.910898	15.567040	-0.056212	4.169731
280.374808	5928.928126	15.572045	-0.056135	4.167031
280.441284	5920.870424	15.577050	-0.056142	4.164308
280.396434	5912.942516	15.582055	-0.056128	4.161627
280.387865	5904.895883	15.587059	-0.056122	4.158904
280.387830	5896.933514	15.592064	-0.056116	4.156208
280.248281	5888.861227	15.597069	-0.056085	4.153471
280.180509	5880.865558	15.602074	-0.056067	4.150759
280.380388	5872.904760	15.607079	-0.056100	4.148060
280.387631	5864.831497	15.612083	-0.056096	4.145320
280.255773	5856.934604	15.617088	-0.056066	4.142635
280.030907	5848.896435	15.622093	-0.056019	4.139900
280.231056	5840.933422	15.627098	-0.056051	4.137194
279.907826	5832.929523	15.632103	-0.055986	4.134465
280.041695	5824.861042	15.637107	-0.056005	4.131719
280.104072	5816.889204	15.642112	-0.056012	4.129002
279.698038	5808.860427	15.647117	-0.055931	4.126259
279.751166	5800.888542	15.652122	-0.055936	4.123539
279.751434	5792.884495	15.657127	-0.055931	4.120805
279.846256	5784.924383	15.662131	-0.055943	4.118086
279.847682	5776.896206	15.667136	-0.055938	4.115340
279.559647	5768.882064	15.672141	-0.055879	4.112594
279.599295	5760.839585	15.677146	-0.055882	4.109841
279.666417	5752.881627	15.682151	-0.055889	4.107114
279.567259	5744.848593	15.687155	-0.055865	4.104359
279.572049	5736.899922	15.692160	-0.055861	4.101631
279.381014	5728.896573	15.697165	-0.055820	4.098881
279.266101	5720.911276	15.702170	-0.055794	4.096136
279.352503	5712.916550	15.707175	-0.055805	4.093388
279.212390	5704.863163	15.712179	-0.055773	4.090615
279.418071	5696.913654	15.717184	-0.055807	4.087881
279.269205	5688.876040	15.722189	-0.055774	4.085110
278.982312	5680.939775	15.727194	-0.055715	4.082370
279.373847	5672.922166	15.732199	-0.055783	4.079609
279.017466	5664.958734	15.737203	-0.055711	4.076855
278.959460	5656.919640	15.742208	-0.055695	4.074077
278.972249	5648.878774	15.747213	-0.055693	4.071298
278.700116	5640.939426	15.752218	-0.055637	4.068548
278.721532	5632.903793	15.757223	-0.055636	4.065766
278.697763	5624.925907	15.762227	-0.055626	4.063002
278.689138	5616.962766	15.767232	-0.055619	4.060242
278.667866	5608.945278	15.772237	-0.055610	4.057461
278.818819	5600.898480	15.777242	-0.055633	4.054669
278.729899	5592.927094	15.782247	-0.055611	4.051899
278.583974	5584.887208	15.787251	-0.055579	4.049103
278.663920	5576.963030	15.792256	-0.055589	4.046347
278.629594	5568.925190	15.797261	-0.055577	4.043549
278.375744	5560.934265	15.802266	-0.055525	4.040762
278.427699	5552.968500	15.807271	-0.055529	4.037986
278.341733	5544.916424	15.812275	-0.055508	4.035177
278.414307	5536.845472	15.817280	-0.055516	4.032361
278.279634	5528.846941	15.822285	-0.055486	4.029565
278.058398	5520.887153	15.827290	-0.055440	4.026779
278.122378	5512.898541	15.832295	-0.055446	4.023986
277.926094	5504.898039	15.837299	-0.055405	4.021183
278.002873	5496.905748	15.842304	-0.055414	4.018385
277.987436	5488.890028	15.847309	-0.055406	4.015575
277.846845	5480.920940	15.852314	-0.055374	4.012778
277.910334	5472.885472	15.857319	-0.055381	4.009958
277.870544	5464.874364	15.862323	-0.055369	4.007144
277.900628	5456.884488	15.867328	-0.055369	4.004336
277.751411	5448.947153	15.872333	-0.055336	4.001541
277.757589	5440.916342	15.877338	-0.055332	3.998715
277.768971	5432.940599	15.882343	-0.055329	3.995906
277.512313	5424.906293	15.887347	-0.055276	3.993070
277.592754	5416.907814	15.892352	-0.055286	3.990249
277.601891	5408.877505	15.897357	-0.055282	3.987415
277.420987	5400.876527	15.902362	-0.055243	3.984586
277.561233	5392.947064	15.907367	-0.055264	3.981785
277.406683	5384.901596	15.912371	-0.055230	3.978937
277.304584	5376.923035	15.917376	-0.055206	3.976111
277.432480	5368.877061	15.922381	-0.055225	3.973262
277.381762	5360.889083	15.927386	-0.055210	3.970430
277.412299	5352.919777	15.932391	-0.055211	3.967603
277.124082	5344.890124	15.937395	-0.055152	3.964748
277.380172	5336.992005	15.942400	-0.055195	3.961946
277.091775	5328.991529	15.947405	-0.055136	3.959097
277.108669	5321.005342	15.952410	-0.055134	3.956256
277.060815	5312.985008	15.957415	-0.055120	3.953400
277.018325	5304.951848	15.962419	-0.055107	3.950537
277.039815	5296.939860	15.967424	-0.055105	3.947680
276.881806	5288.902046	15.972429	-0.055071	3.944810
276.810840	5280.965603	15.977434	-0.055052	3.941975
276.768361	5272.988986	15.982439	-0.055039	3.939124
276.529906	5264.993647	15.987443	-0.054990	3.936260
276.561662	5256.975363	15.992448	-0.054990	3.933392
276.665421	5248.916695	15.997453	-0.055005	3.930507
276.536317	5240.958950	16.002458	-0.054975	3.927653
276.389646	5232.982681	16.007463	-0.054943	3.924790
276.453558	5225.006219	16.012467	-0.054950	3.921928
276.584233	5217.004432	16.017472	-0.054969	3.919057
276.401229	5208.997205	16.022477	-0.054930	3.916176
276.541743	5200.961521	16.027482	-0.054951	3.913288
276.670044	5192.941868	16.032487	-0.054969	3.910403
276.318941	5184.960095	16.037491	-0.054899	3.907522
276.175779	5176.969495	16.042496	-0.054867	3.904639
276.256004	5169.002908	16.047501	-0.054877	3.901766
276.148104	5160.974837	16.052506	-0.054851	3.898866
276.116255	5153.030088	16.057511	-0.054840	3.895995
275.958109	5144.994141	16.062515	-0.054806	3.893086
276.174407	5136.915597	16.067520	-0.054841	3.890167
275.797932	5129.019436	16.072525	-0.054766	3.887301
275.677697	5120.975545	16.077530	-0.054738	3.884384
275.918768	5113.004928	16.082535	-0.054778	3.881498
275.859477	5104.988825	16.087539	-0.054762	3.878587
275.764386	5097.028776	16.092544	-0.054739	3.875694
275.979545	5088.826491	16.097549	-0.054773	3.872717
275.825768	5080.784700	16.102554	-0.054740	3.869789
275.676089	5072.897167	16.107559	-0.054707	3.866915
275.446985	5064.924721	16.112563	-0.054659	3.864006
275.572459	5056.964191	16.117568	-0.054677	3.861107
275.336000	5048.959790	16.122573	-0.054628	3.858182
275.194984	5040.992311	16.127578	-0.054596	3.855270
275.407087	5032.959673	16.132583	-0.054631	3.852339
275.294549	5024.939635	16.137587	-0.054605	3.849404
275.098184	5017.007096	16.142592	-0.054563	3.846497
275.073884	5008.993672	16.147597	-0.054553	3.843562
275.222380	5001.020308	16.152602	-0.054576	3.840642
275.124397	4993.070807	16.157607	-0.054552	3.837724
274.884430	4984.998388	16.162611	-0.054502	3.834756
275.255753	4977.007088	16.167616	-0.054566	3.831828
275.156900	4969.014014	16.172621	-0.054543	3.828887
275.012888	4961.004212	16.177626	-0.054511	3.825938
275.000177	4953.078037	16.182631	-0.054503	3.823019
275.003747	4945.021504	16.187635	-0.054499	3.820050
274.928371	4937.079793	16.192640	-0.054480	3.817120
274.766607	4929.059490	16.197645	-0.054444	3.814156
274.635781	4921.054719	16.202650	-0.054415	3.811197
274.612173	4913.061077	16.207655	-0.054405	3.808242
274.526068	4905.048558	16.212659	-0.054384	3.805276
274.748246	4897.131648	16.217664	-0.054420	3.802350
274.430678	4889.096918	16.222669	-0.054356	3.799366
274.554751	4881.095244	16.227674	-0.054374	3.796401
274.390441	4873.091304	16.232679	-0.054338	3.793428
274.386679	4865.011248	16.237683	-0.054332	3.790427
274.180792	4857.066978	16.242688	-0.054289	3.787470
274.089143	4849.044275	16.247693	-0.054267	3.784484
274.224610	4841.073256	16.252698	-0.054287	3.781519
274.163755	4833.107471	16.257703	-0.054270	3.778550
273.852607	4825.079958	16.262707	-0.054207	3.775550
274.210082	4817.085263	16.267712	-0.054268	3.772575
273.961138	4809.070243	16.272717	-0.054217	3.769576
273.813943	4801.079003	16.277722	-0.054184	3.766586
273.787796	4793.106932	16.282727	-0.054174	3.763604
273.705904	4785.058690	16.287731	-0.054154	3.760589
273.710621	4777.130826	16.292736	-0.054150	3.757619
273.654058	4769.098920	16.297741	-0.054134	3.754607
273.749070	4761.069259	16.302746	-0.054146	3.751596
273.866007	4753.077910	16.307751	-0.054163	3.748597
273.530015	4745.045088	16.312755	-0.054095	3.745571
273.422122	4737.142624	16.317760	-0.054070	3.742596
273.334117	4729.119263	16.322765	-0.054048	3.739573
273.305316	4721.156755	16.327770	-0.054038	3.736573
273.514472	4713.120518	16.332775	-0.054072	3.733547
273.364070	4705.080001	16.337779	-0.054038	3.730510
273.356252	4697.103311	16.342784	-0.054032	3.727497
273.286478	4689.095677	16.347789	-0.054014	3.724469
273.425811	4681.202731	16.352794	-0.054035	3.721486
273.438761	4673.168225	16.357799	-0.054032	3.718445
273.283715	4665.189620	16.362803	-0.053998	3.715418
273.380572	4657.119327	16.367808	-0.054011	3.712360
273.287537	4649.080879	16.372813	-0.053988	3.709307
273.163301	4641.087236	16.377818	-0.053960	3.706268
273.025208	4633.160205	16.382823	-0.053929	3.703251
272.865043	4625.124641	16.387827	-0.053894	3.700190
272.907797	4617.182730	16.392832	-0.053897	3.697167
272.872375	4609.150806	16.397837	-0.053885	3.694105
272.982093	4601.163620	16.402842	-0.053900	3.691061
272.881063	4593.208932	16.407847	-0.053876	3.688022
272.629564	4585.160377	16.412851	-0.053824	3.684941
272.651680	4577.224036	16.417856	-0.053823	3.681907
272.581095	4569.223651	16.422861	-0.053805	3.678844
272.592081	4561.218902	16.427866	-0.053802	3.675779
272.395589	4553.232881	16.432871	-0.053760	3.672712
272.426463	4545.167006	16.437875	-0.053761	3.669619
272.444825	4537.233107	16.442880	-0.053759	3.666573
272.429561	4529.213021	16.447885	-0.053751	3.663491
272.349462	4521.221062	16.452890	-0.053731	3.660415
272.445729	4513.259735	16.457895	-0.053744	3.657353
272.255672	4505.246486	16.462899	-0.053703	3.654261
272.326939	4497.212004	16.467904	-0.053711	3.651165
272.225949	4489.223431	16.472909	-0.053687	3.648079
271.993846	4481.224686	16.477914	-0.053639	3.644984
272.103824	4473.290354	16.482919	-0.053654	3.641919
271.824785	4465.288313	16.487923	-0.053597	3.638816
272.113464	4457.285904	16.492928	-0.053646	3.635725
271.902920	4449.220481	16.497933	-0.053601	3.632594
271.709345	4441.231746	16.502938	-0.053560	3.629490
271.822748	4433.247290	16.507943	-0.053576	3.626393
271.607594	4425.278641	16.512947	-0.053531	3.623291
271.706710	4417.281516	16.517952	-0.053544	3.620184
271.734258	4409.275343	16.522957	-0.053544	3.617068
271.654129	4401.277150	16.527962	-0.053524	3.613950
271.689512	4393.293043	16.532967	-0.053525	3.610838
271.751664	4385.273150	16.537971	-0.053532	3.607710
271.790384	4377.263434	16.542976	-0.053534	3.604583
271.548157	4369.357874	16.547981	-0.053483	3.601486
271.402655	4361.354294	16.552986	-0.053451	3.598351
271.545068	4353.352518	16.557991	-0.053473	3.595221
271.248617	4345.347405	16.562995	-0.053412	3.592075
271.277816	4337.363650	16.568000	-0.053412	3.588944
271.261311	4329.331301	16.573005	-0.053404	3.585790
271.131480	4321.379262	16.578010	-0.053375	3.582662
271.224944	4313.380122	16.583015	-0.053387	3.579518
271.146058	4305.401169	16.588019	-0.053367	3.576375
271.290114	4297.386254	16.593024	-0.053389	3.573221
271.022781	4289.363021	16.598029	-0.053334	3.570049
270.922330	4281.392650	16.603034	-0.053310	3.566901
271.032269	4273.417222	16.608039	-0.053325	3.563753
270.742794	4265.425055	16.613043	-0.053266	3.560584
270.777237	4257.440102	16.618048	-0.053268	3.557425
270.777480	4249.375719	16.623053	-0.053262	3.554231
270.702927	4241.281589	16.628058	-0.053243	3.551020
270.665300	4233.340723	16.633063	-0.053231	3.547867
270.540547	4225.345024	16.638067	-0.053203	3.544688
270.632623	4217.405643	16.643072	-0.053215	3.541534
270.503403	4209.413668	16.648077	-0.053186	3.538350
270.312771	4201.422556	16.653082	-0.053145	3.535162
270.524919	4193.421966	16.658087	-0.053179	3.531979
270.464763	4185.391012	16.663091	-0.053163	3.528773
270.393436	4177.408082	16.668096	-0.053144	3.525583
270.403420	4169.457522	16.673101	-0.053141	3.522406
270.245701	4161.456594	16.678106	-0.053107	3.519200
270.164930	4153.492280	16.683111	-0.053086	3.516008
270.067456	4145.457091	16.688115	-0.053063	3.512785
270.048358	4137.454481	16.693120	-0.053054	3.509574
269.916576	4129.468579	16.698125	-0.053025	3.506363
270.034491	4121.474849	16.703130	-0.053041	3.503154
270.151293	4113.484601	16.708135	-0.053058	3.499944
269.943296	4105.507222	16.713139	-0.053014	3.496725
269.919852	4097.503712	16.718144	-0.053005	3.493499
269.918008	4089.504396	16.723149	-0.052999	3.490272
269.665187	4081.556650	16.728154	-0.052947	3.487055
269.501686	4073.560781	16.733159	-0.052911	3.483818
269.365562	4065.557950	16.738163	-0.052881	3.480577
269.545995	4057.606537	16.743168	-0.052909	3.477363
269.560197	4049.566060	16.748173	-0.052907	3.474105
269.291362	4041.545317	16.753178	-0.052851	3.470843
269.533006	4033.560519	16.758183	-0.052891	3.467608
269.432858	4025.548571	16.763187	-0.052867	3.464349
269.413583	4017.619138	16.768192	-0.052859	3.461123
269.247296	4009.596097	16.773197	-0.052823	3.457851
269.169026	4001.590590	16.778202	-0.052803	3.454585
269.057483	3993.638177	16.783207	-0.052777	3.451337
268.844228	3985.613537	16.788211	-0.052732	3.448054
268.940668	3977.602419	16.793216	-0.052745	3.444782
268.818228	3969.664470	16.798221	-0.052717	3.441531
268.742348	3961.635091	16.803226	-0.052698	3.438240
268.591127	3953.671275	16.808231	-0.052664	3.434971
268.711611	3945.617121	16.813235	-0.052681	3.431670
268.645470	3937.641998	16.818240	-0.052664	3.428393
268.798235	3929.624134	16.823245	-0.052687	3.425102
268.731993	3921.662815	16.828250	-0.052670	3.421824
268.587904	3913.689748	16.833255	-0.052638	3.418535
268.335147	3905.686379	16.838259	-0.052586	3.415227
268.503637	3897.711579	16.843264	-0.052612	3.411942
268.636303	3889.672540	16.848269	-0.052631	3.408626
268.540685	3881.683452	16.853274	-0.052608	3.405319
268.261591	3873.794215	16.858279	-0.052551	3.402044
268.420453	3865.748441	16.863283	-0.052576	3.398717
268.341310	3857.782881	16.868288	-0.052556	3.395411
268.248391	3849.703729	16.873293	-0.052533	3.392054
268.227878	3841.664143	16.878298	-0.052524	3.388713
268.343478	3833.710420	16.883303	-0.052541	3.385409
268.121864	3825.761148	16.888307	-0.052494	3.382092
268.037209	3817.761122	16.893312	-0.052473	3.378755
268.071211	3809.782259	16.898317	-0.052474	3.375428
268.013585	3801.792068	16.903322	-0.052459	3.372089
267.990376	3793.788997	16.908327	-0.052449	3.368744
267.998536	3785.790492	16.913331	-0.052445	3.365397
267.962546	3777.838707	16.918336	-0.052434	3.362066
267.764621	3769.850537	16.923341	-0.052392	3.358710
267.623875	3761.873012	16.928346	-0.052360	3.355357
267.745406	3753.856612	16.933351	-0.052378	3.351994
267.637680	3745.824049	16.938355	-0.052352	3.348613
267.539885	3737.858111	16.943360	-0.052329	3.345256
267.440677	3729.929224	16.948365	-0.052305	3.341912
267.409412	3721.877432	16.953370	-0.052294	3.338515
267.359699	3713.909359	16.958375	-0.052280	3.335149
266.983620	3705.945133	16.963379	-0.052205	3.331770
266.957938	3697.937369	16.968384	-0.052195	3.328381
267.099941	3689.887821	16.973389	-0.052216	3.324977
267.008619	3681.944083	16.978394	-0.052194	3.321607
267.020110	3673.967119	16.983399	-0.052191	3.318222
266.883398	3665.959849	16.988403	-0.052160	3.314816
266.952778	3657.940590	16.993408	-0.052168	3.311408
267.134272	3649.925559	16.998413	-0.052197	3.308003
266.967061	3641.942114	17.003418	-0.052160	3.304595
266.926564	3634.005541	17.008423	-0.052148	3.301209
266.795534	3626.014263	17.013427	-0.052118	3.297792
266.720353	3618.016889	17.018432	-0.052099	3.294371
266.812846	3610.003469	17.023437	-0.052111	3.290945
266.730724	3602.005901	17.028442	-0.052091	3.287517
266.680909	3594.044400	17.033447	-0.052076	3.284101
266.590423	3586.063588	17.038451	-0.052054	3.280673
266.520472	3578.106756	17.043456	-0.052036	3.277251
266.616497	3570.079506	17.048461	-0.052049	3.273802
266.372979	3562.070974	17.053466	-0.051998	3.270345
266.112901	3554.145649	17.058471	-0.051945	3.266919
266.353826	3546.089414	17.063475	-0.051984	3.263452
266.135873	3538.127310	17.068480	-0.051939	3.260004
266.410678	3530.114520	17.073485	-0.051985	3.256550
266.415550	3522.112340	17.078490	-0.051980	3.253087
266.424511	3514.087346	17.083495	-0.051977	3.249610
266.165376	3506.139342	17.088499	-0.051923	3.246152
266.377776	3498.156715	17.093504	-0.051958	3.242694
266.237185	3490.179755	17.098509	-0.051926	3.239221
266.055846	3482.205853	17.103514	-0.051888	3.235743
265.982848	3474.191227	17.108519	-0.051869	3.232249
265.831160	3466.173979	17.113523	-0.051835	3.228746
265.967737	3458.170252	17.118528	-0.051856	3.225258
265.834157	3450.218763	17.123533	-0.051826	3.221777
265.782818	3442.206241	17.128538	-0.051811	3.218269
265.660849	3434.253235	17.133543	-0.051783	3.214780
265.463558	3426.263304	17.138547	-0.051741	3.211269
265.686189	3418.254276	17.143552	-0.051777	3.207762
265.552122	3410.262510	17.148557	-0.051747	3.204245
265.385211	3402.305372	17.153562	-0.051711	3.200737
265.327345	3394.353856	17.158567	-0.051695	3.197233
265.324770	3386.323778	17.163571	-0.051689	3.193692
265.426105	3378.291367	17.168576	-0.051703	3.190151
265.253763	3370.351670	17.173581	-0.051666	3.186635
265.120456	3362.352226	17.178586	-0.051636	3.183091
265.229124	3354.388049	17.183591	-0.051651	3.179568
265.217761	3346.368793	17.188595	-0.051644	3.176012
265.116297	3338.388225	17.193600	-0.051620	3.172465
265.007113	3330.405438	17.198605	-0.051594	3.168914
264.803702	3322.412644	17.203610	-0.051551	3.165349
264.798375	3314.465259	17.208615	-0.051545	3.161809
264.880635	3306.441363	17.213619	-0.051555	3.158235
265.095564	3298.439567	17.218624	-0.051590	3.154673
264.790713	3290.454394	17.223629	-0.051528	3.151091
264.845619	3282.438702	17.228634	-0.051533	3.147508
264.900031	3274.489288	17.233639	-0.051538	3.143949
264.571544	3266.505392	17.238643	-0.051472	3.140355
264.456194	3258.555200	17.243648	-0.051445	3.136781
264.667147	3250.521848	17.248653	-0.051479	3.133180
264.758411	3242.492704	17.253658	-0.051491	3.129571
264.654463	3234.555651	17.258663	-0.051467	3.125991
264.391315	3226.601882	17.263667	-0.051412	3.122392
264.497914	3218.585068	17.268672	-0.051427	3.118777
264.203822	3210.624631	17.273677	-0.051367	3.115166
264.312912	3202.592346	17.278682	-0.051382	3.111536
264.372421	3194.616302	17.283687	-0.051388	3.107924
263.970153	3186.664384	17.288691	-0.051308	3.104299
263.954085	3178.671872	17.293696	-0.051300	3.100668
263.918334	3170.704418	17.298701	-0.051288	3.097044
264.089547	3162.662588	17.303706	-0.051315	3.093391
263.903028	3154.678969	17.308711	-0.051275	3.089744
263.889164	3146.715603	17.313715	-0.051267	3.086110
263.990499	3138.728202	17.318720	-0.051281	3.082465
263.988456	3130.740817	17.323725	-0.051275	3.078812
263.609429	3122.795473	17.328730	-0.051200	3.075156
263.853415	3114.702923	17.333735	-0.051240	3.071457
263.804000	3106.694557	17.338739	-0.051226	3.067779
263.820140	3098.751636	17.343744	-0.051223	3.064129
263.816796	3090.791671	17.348749	-0.051218	3.060466
263.571537	3082.816423	17.353754	-0.051167	3.056781
263.437529	3074.837545	17.358759	-0.051137	3.053094
263.336191	3066.821120	17.363763	-0.051113	3.049388
263.477935	3058.860466	17.368768	-0.051134	3.045714
263.296087	3050.919622	17.373773	-0.051095	3.042029
262.994276	3042.941583	17.378778	-0.051034	3.038317
263.157469	3034.945744	17.383783	-0.051059	3.034614
263.141714	3026.908874	17.388787	-0.051051	3.030880
263.031199	3018.939334	17.393792	-0.051025	3.027167
263.042518	3010.981752	17.398797	-0.051022	3.023461
262.870009	3002.977389	17.403802	-0.050985	3.019720
262.982127	2995.015599	17.408807	-0.051000	3.016008
262.828716	2986.989093	17.413811	-0.050967	3.012248
262.858756	2979.004209	17.418816	-0.050967	3.008512
262.839753	2971.019710	17.423821	-0.050958	3.004769
262.595120	2963.082761	17.428826	-0.050908	3.001033
262.611891	2955.109144	17.433831	-0.050906	2.997287
262.700694	2947.079550	17.438835	-0.050917	2.993514
262.422488	2939.078810	17.443840	-0.050860	2.989732
262.420818	2931.112092	17.448845	-0.050855	2.985974
262.591027	2923.102881	17.453850	-0.050881	2.982201
262.672857	2915.149371	17.458855	-0.050891	2.978445
262.359415	2907.185833	17.463859	-0.050828	2.974659
262.385408	2899.189943	17.468864	-0.050827	2.970870
262.351272	2891.217217	17.473869	-0.050816	2.967084
262.298098	2883.219951	17.478874	-0.050801	2.963281
262.350989	2875.241317	17.483879	-0.050805	2.959487
262.165971	2867.300321	17.488883	-0.050766	2.955694
262.033380	2859.290747	17.493888	-0.050736	2.951866
262.229769	2851.294170	17.498893	-0.050767	2.948057
262.158631	2843.287048	17.503898	-0.050749	2.944223
262.204131	2835.324069	17.508903	-0.050752	2.940412
261.895591	2827.367347	17.513907	-0.050690	2.936580
261.741849	2819.382981	17.518912	-0.050656	2.932738
261.810279	2811.380532	17.523917	-0.050664	2.928894
261.766741	2803.377384	17.528922	-0.050650	2.925039
261.927209	2795.441573	17.533927	-0.050675	2.921221
261.800025	2787.466610	17.538931	-0.050646	2.917365
261.663433	2779.454878	17.543936	-0.050616	2.913485
261.478083	2771.421838	17.548941	-0.050576	2.909588
261.355255	2763.444954	17.553946	-0.050548	2.905715
261.274654	2755.521709	17.558951	-0.050528	2.901866
261.052892	2747.539796	17.563955	-0.050481	2.897975
261.204147	2739.541734	17.568960	-0.050504	2.894091
261.154727	2731.549581	17.573965	-0.050490	2.890194
261.080268	2723.563330	17.578970	-0.050471	2.886294
261.108826	2715.642917	17.583975	-0.050471	2.882425
261.081545	2707.643021	17.588979	-0.050461	2.878510
261.211274	2699.656955	17.593984	-0.050480	2.874605
261.139471	2691.637967	17.598989	-0.050461	2.870667
261.007580	2683.675464	17.603994	-0.050432	2.866748
261.032451	2675.685476	17.608999	-0.050431	2.862819
261.000071	2667.720452	17.614003	-0.050420	2.858894
260.775900	2659.753100	17.619008	-0.050373	2.854952
260.787705	2651.753952	17.624013	-0.050370	2.851001
260.757128	2643.759931	17.629018	-0.050359	2.847045
260.708803	2635.829425	17.634023	-0.050345	2.843114
260.748050	2627.841532	17.639027	-0.050347	2.839154
260.570473	2619.893050	17.644032	-0.050309	2.835196
260.598511	2611.874142	17.649037	-0.050309	2.831209
260.562149	2603.878832	17.654042	-0.050297	2.827224
260.447904	2595.919928	17.659047	-0.050271	2.823248
260.287694	2587.941934	17.664051	-0.050236	2.819254
260.178458	2579.981369	17.669056	-0.050210	2.815265
260.442726	2571.940271	17.674061	-0.050254	2.811252
260.238346	2563.984666	17.679066	-0.050211	2.807250
260.375114	2556.023767	17.684071	-0.050231	2.803258
260.136111	2548.065192	17.689075	-0.050182	2.799240
260.227734	2540.090670	17.694080	-0.050194	2.795228
260.061332	2532.100390	17.699085	-0.050157	2.791187
259.981091	2524.119239	17.704090	-0.050137	2.787149
259.782529	2516.178172	17.709095	-0.050095	2.783120
259.493700	2508.211150	17.714099	-0.050036	2.779065
259.571841	2500.226254	17.719104	-0.050046	2.775018
259.585203	2492.208929	17.724109	-0.050043	2.770944
259.539147	2484.228690	17.729114	-0.050029	2.766879
259.570919	2476.265816	17.734119	-0.050030	2.762822
259.453319	2468.299674	17.739123	-0.050003	2.758749
259.622217	2460.313070	17.744128	-0.050029	2.754676
259.440306	2452.262907	17.749133	-0.049990	2.750543
259.268601	2444.313180	17.754138	-0.049953	2.746456
259.249191	2436.355047	17.759143	-0.049944	2.742368
259.065990	2428.396535	17.764147	-0.049905	2.738264
259.090104	2420.420758	17.769152	-0.049904	2.734157
259.179107	2412.401508	17.774157	-0.049916	2.730026
259.140665	2404.431767	17.779162	-0.049904	2.725906
258.990633	2396.517468	17.784167	-0.049870	2.721802
258.934172	2388.546287	17.789171	-0.049855	2.717668
258.951375	2380.546648	17.794176	-0.049853	2.713517
258.740523	2372.584001	17.799181	-0.049808	2.709365
258.608781	2364.601468	17.804186	-0.049779	2.705202
258.824808	2356.630425	17.809191	-0.049814	2.701059
258.575606	2348.688938	17.814195	-0.049762	2.696896
258.516036	2340.700135	17.819200	-0.049746	2.692714
258.691129	2332.680111	17.824205	-0.049773	2.688524
258.659442	2324.711629	17.829210	-0.049762	2.684342
258.398195	2316.805798	17.834215	-0.049709	2.680171
258.348811	2308.848326	17.839219	-0.049694	2.675980
258.485215	2300.796852	17.844224	-0.049715	2.671745
258.255475	2292.841387	17.849229	-0.049667	2.667530
258.295758	2284.826947	17.854234	-0.049669	2.663295
258.397239	2276.880232	17.859239	-0.049683	2.659093
258.262973	2268.915298	17.864243	-0.049653	2.654859
257.978480	2260.959430	17.869248	-0.049594	2.650613
258.187405	2252.958898	17.874253	-0.049628	2.646369
258.001278	2245.005606	17.879258	-0.049588	2.642118
258.040054	2237.062522	17.884263	-0.049590	2.637880
257.810268	2229.090144	17.889267	-0.049542	2.633602
258.126994	2221.046265	17.894272	-0.049596	2.629314
258.067270	2213.101450	17.899277	-0.049580	2.625048
257.668392	2205.161441	17.904282	-0.049501	2.620755
257.875417	2197.202509	17.909287	-0.049534	2.616485
257.761350	2189.214831	17.914291	-0.049508	2.612171
257.603012	2181.248780	17.919296	-0.049473	2.607858
257.607707	2173.289625	17.924301	-0.049469	2.603553
257.438282	2165.339915	17.929306	-0.049432	2.599235
257.580469	2157.372520	17.934311	-0.049453	2.594920
257.336508	2149.206167	17.939315	-0.049403	2.590464
257.301325	2141.255940	17.944320	-0.049391	2.586132
257.325955	2133.319869	17.949325	-0.049390	2.581805
256.913715	2125.410078	17.954330	-0.049309	2.577455
257.166558	2117.429386	17.959335	-0.049350	2.573104
256.976937	2109.471206	17.964339	-0.049310	2.568728
256.931682	2101.494347	17.969344	-0.049296	2.564344
256.924306	2093.563522	17.974349	-0.049290	2.559981
256.938099	2085.587510	17.979354	-0.049287	2.555587
257.179073	2077.599900	17.984359	-0.049327	2.551194
256.768965	2069.664538	17.989363	-0.049246	2.546777
256.753739	2061.701041	17.994368	-0.049238	2.542365
256.669178	2053.756516	17.999373	-0.049217	2.537951
256.658838	2045.751896	18.004378	-0.049210	2.533500
256.612419	2037.800662	18.009383	-0.049196	2.529070
256.505711	2029.843951	18.014387	-0.049171	2.524623
256.245214	2021.925973	18.019392	-0.049117	2.520180
256.293903	2013.949984	18.024397	-0.049121	2.515719
256.270031	2005.934270	18.029402	-0.049112	2.511222
256.257308	1997.974245	18.034407	-0.049104	2.506749
256.022331	1990.010421	18.039411	-0.049055	2.502250
255.982035	1982.046527	18.044416	-0.049042	2.497757
256.179183	1974.042648	18.049421	-0.049074	2.493250
256.133867	1966.060692	18.054426	-0.049060	2.488730
255.944821	1958.140442	18.059431	-0.049020	2.484226
255.903015	1950.196115	18.064435	-0.049007	2.479711
255.943135	1942.243323	18.069440	-0.049009	2.475189
255.888845	1934.257914	18.074445	-0.048994	2.470634
255.798275	1926.278869	18.079450	-0.048972	2.466070
255.803223	1918.344732	18.084455	-0.048968	2.461531
255.553156	1910.403506	18.089459	-0.048916	2.456961
255.676604	1902.415671	18.094464	-0.048934	2.452383
255.715439	1894.440719	18.099469	-0.048936	2.447798
255.494231	1886.495254	18.104474	-0.048890	2.443201
255.503637	1878.560012	18.109479	-0.048887	2.438619
255.425320	1870.583268	18.114483	-0.048867	2.433998
255.151003	1862.571634	18.119488	-0.048811	2.429333
254.860581	1854.640778	18.124493	-0.048751	2.424705
254.808384	1846.693544	18.129498	-0.048736	2.420076
255.175273	1838.689047	18.134503	-0.048800	2.415437
254.920460	1830.741638	18.139507	-0.048747	2.410775
255.050782	1822.758454	18.144512	-0.048766	2.406113
254.839016	1814.847219	18.149517	-0.048722	2.401457
254.831395	1806.896720	18.154522	-0.048715	2.396785
254.926850	1798.912504	18.159527	-0.048728	2.392092
254.868345	1790.941407	18.164531	-0.048712	2.387385
254.494777	1783.023102	18.169536	-0.048637	2.382676
254.705531	1775.054160	18.174541	-0.048671	2.377973
254.617931	1767.079544	18.179546	-0.048650	2.373234
254.593789	1759.118692	18.184551	-0.048640	2.368499
254.539026	1751.163742	18.189555	-0.048625	2.363755
254.393923	1743.255743	18.194560	-0.048592	2.359022
254.384599	1735.297708	18.199565	-0.048586	2.354261
254.219356	1727.305766	18.204570	-0.048550	2.349458
254.204021	1719.343518	18.209575	-0.048542	2.344674
254.013472	1711.411108	18.214579	-0.048501	2.339884
253.797730	1703.490710	18.219584	-0.048456	2.335090
254.113007	1695.464120	18.224589	-0.048509	2.330265
254.129899	1687.493426	18.229594	-0.048507	2.325440
254.075750	1679.587719	18.234599	-0.048492	2.320638
253.864656	1671.671567	18.239603	-0.048448	2.315806
253.795132	1663.674964	18.244608	-0.048430	2.310928
253.841084	1655.717557	18.249613	-0.048433	2.306072
253.766869	1647.766294	18.254618	-0.048414	2.301200
253.525258	1639.848989	18.259623	-0.048364	2.296325
253.703331	1631.860888	18.264627	-0.048392	2.291430
253.753575	1623.882214	18.269632	-0.048396	2.286521
253.632048	1615.967754	18.274637	-0.048368	2.281626
253.445923	1608.051265	18.279642	-0.048329	2.276713
253.385100	1600.053693	18.284647	-0.048312	2.271750
253.139257	1592.080862	18.289651	-0.048261	2.266776
253.084103	1584.132869	18.294656	-0.048246	2.261823
253.214922	1576.187293	18.299661	-0.048265	2.256876
253.024048	1568.242818	18.304666	-0.048224	2.251892
252.966006	1560.289141	18.309671	-0.048208	2.246902
253.171393	1552.311548	18.314675	-0.048241	2.241909
253.089586	1544.396035	18.319680	-0.048221	2.236919
253.036117	1536.445591	18.324685	-0.048206	2.231898
252.970307	1528.480757	18.329690	-0.048189	2.226855
253.007744	1520.553256	18.334695	-0.048190	2.221834
252.772526	1512.635928	18.339699	-0.048142	2.216784
252.682220	1504.678752	18.344704	-0.048120	2.211710
252.618574	1496.746648	18.349709	-0.048103	2.206642
252.446261	1488.806152	18.354714	-0.048065	2.201547
252.435041	1480.880665	18.359719	-0.048058	2.196465
252.358787	1472.920572	18.364723	-0.048039	2.191343
252.116576	1464.957787	18.369728	-0.047989	2.186192
252.120744	1457.029793	18.374733	-0.047984	2.181074
251.967220	1449.087791	18.379738	-0.047951	2.175920
252.078729	1441.112932	18.384743	-0.047966	2.170757
251.934307	1433.182744	18.389747	-0.047934	2.165587
251.738719	1425.267854	18.394752	-0.047893	2.160410
251.943125	1417.301020	18.399757	-0.047926	2.155224
251.824400	1409.349521	18.404762	-0.047898	2.150005
251.624031	1401.445679	18.409767	-0.047856	2.144797
251.787020	1393.463014	18.414771	-0.047881	2.139559
251.863685	1385.518264	18.419776	-0.047890	2.134324
251.930087	1377.571298	18.424781	-0.047897	2.129075
251.357156	1369.718718	18.429786	-0.047786	2.123814
251.615748	1361.749576	18.434791	-0.047829	2.118542
251.597133	1353.781468	18.439795	-0.047820	2.113230
251.196877	1345.838221	18.444800	-0.047740	2.107886
251.203638	1337.917876	18.449805	-0.047737	2.102582
251.466634	1329.933086	18.454810	-0.047780	2.097247
251.242359	1322.033127	18.459815	-0.047733	2.091907
251.156510	1314.089763	18.464819	-0.047712	2.086538
251.120031	1306.180462	18.469824	-0.047700	2.081183
251.240467	1298.252175	18.474829	-0.047718	2.075817
251.119595	1290.292965	18.479834	-0.047690	2.070392
251.183593	1282.359075	18.484839	-0.047697	2.064989
251.170120	1274.448745	18.489843	-0.047689	2.059579
250.939193	1266.540460	18.494848	-0.047641	2.054135
250.895899	1258.602261	18.499853	-0.047628	2.048675
250.782154	1250.679945	18.504858	-0.047602	2.043204
250.652812	1242.782554	18.509863	-0.047572	2.037734
250.521166	1234.839959	18.514867	-0.047543	2.032218
250.460938	1226.889435	18.519872	-0.047526	2.026688
250.603012	1218.946957	18.524877	-0.047548	2.021170
250.198566	1211.070902	18.529882	-0.047467	2.015626
250.051615	1203.152091	18.534887	-0.047435	2.010064
250.124681	1195.209896	18.539891	-0.047443	2.004493
249.818055	1187.335273	18.544896	-0.047381	1.998914
249.751742	1179.416782	18.549901	-0.047364	1.993314
249.659404	1171.448513	18.554906	-0.047341	1.987660
249.852469	1163.480962	18.559911	-0.047372	1.982020
249.873982	1155.552457	18.564915	-0.047371	1.976374
249.608217	1147.679761	18.569920	-0.047317	1.970721
249.923523	1139.697477	18.574925	-0.047370	1.965036
249.744171	1131.821870	18.579930	-0.047332	1.959357
249.781554	1123.895054	18.584935	-0.047333	1.953649
249.641627	1115.945438	18.589939	-0.047302	1.947888
249.237308	1108.070681	18.594944	-0.047222	1.942135
249.259949	1100.156315	18.599949	-0.047221	1.936383
249.352619	1092.197180	18.604954	-0.047233	1.930589
249.266272	1084.291546	18.609959	-0.047212	1.924797
249.088332	1076.416541	18.614963	-0.047174	1.919000
249.084602	1068.477104	18.619968	-0.047168	1.913157
249.413710	1060.510966	18.624973	-0.047224	1.907313
249.109756	1052.643445	18.629978	-0.047162	1.901454
249.116565	1044.724362	18.634983	-0.047158	1.895573
249.066144	1036.816320	18.639987	-0.047144	1.889676
249.035640	1028.906382	18.644992	-0.047133	1.883761
248.888209	1021.042593	18.649997	-0.047101	1.877849
248.770767	1013.135889	18.655002	-0.047074	1.871889
248.761604	1005.206735	18.660007	-0.047067	1.865905
248.819388	997.281853	18.665011	-0.047072	1.859913
248.890994	989.367788	18.670016	-0.047081	1.853912
248.864482	981.470123	18.675021	-0.047071	1.847893
248.546313	973.622270	18.680026	-0.047006	1.841857
248.252528	965.761280	18.685031	-0.046947	1.835794
248.320998	957.822427	18.690035	-0.046954	1.829695
248.239739	949.922475	18.695040	-0.046934	1.823586
248.183314	942.030713	18.700045	-0.046918	1.817467
247.997901	934.135297	18.705050	-0.046879	1.811309
247.901933	926.238662	18.710055	-0.046856	1.805139
248.096108	918.328404	18.715059	-0.046887	1.798973
247.896732	910.432718	18.720064	-0.046845	1.792749
248.048931	902.479065	18.725069	-0.046868	1.786501
247.803745	894.610169	18.730074	-0.046817	1.780249
247.841341	886.734794	18.735079	-0.046819	1.774005
247.763670	878.835329	18.740083	-0.046799	1.767705
247.608385	870.969895	18.745088	-0.046765	1.761400
247.571484	863.106299	18.750093	-0.046753	1.755088
247.435507	855.203393	18.755098	-0.046723	1.748710
247.519442	847.314702	18.760103	-0.046734	1.742348
247.397483	839.448865	18.765107	-0.046706	1.735955
247.271339	831.551078	18.770112	-0.046677	1.729511
247.498852	823.651538	18.775117	-0.046714	1.723087
247.122656	815.840468	18.780122	-0.046639	1.716635
246.910640	807.970791	18.785127	-0.046595	1.710130
247.033446	800.054163	18.790131	-0.046613	1.703606
246.871421	792.198310	18.795136	-0.046577	1.697069
246.780522	784.328103	18.800141	-0.046555	1.690505
246.720092	776.442675	18.805146	-0.046539	1.683906
246.810343	768.568403	18.810151	-0.046551	1.677311
246.637868	760.703876	18.815155	-0.046513	1.670663
246.717134	752.809290	18.820160	-0.046523	1.663997
246.887466	744.944580	18.825165	-0.046550	1.657341
246.686890	737.084865	18.830170	-0.046507	1.650613
246.562761	729.254998	18.835175	-0.046479	1.643893
246.524277	721.402062	18.840179	-0.046467	1.637137
246.246492	713.528201	18.845184	-0.046410	1.630302
246.175177	705.668976	18.850189	-0.046392	1.623480
246.241447	697.789830	18.855194	-0.046399	1.616630
246.478985	689.892990	18.860199	-0.046438	1.609761
246.247207	682.078343	18.865203	-0.046390	1.602867
246.122915	674.257624	18.870208	-0.046362	1.595954
246.142281	666.395878	18.875213	-0.046360	1.588995
245.954566	658.559418	18.880218	-0.046320	1.581998
245.819125	650.750557	18.885223	-0.046290	1.575002
245.807174	642.884173	18.890227	-0.046283	1.567941
245.585905	635.083328	18.895232	-0.046236	1.560876
245.743695	627.224180	18.900237	-0.046261	1.553783
245.566870	619.375046	18.905242	-0.046223	1.546616
245.641004	611.531965	18.910247	-0.046231	1.539459
245.363252	603.738350	18.915251	-0.046175	1.532261
244.934759	595.958805	18.920256	-0.046090	1.525020
245.322427	588.065584	18.925261	-0.046157	1.517762
245.269263	580.222500	18.930266	-0.046142	1.510448
244.871818	572.464504	18.935271	-0.046063	1.503127
245.053756	564.614538	18.940275	-0.046092	1.495771
244.897266	556.801494	18.945280	-0.046058	1.488362
244.819027	549.011692	18.950285	-0.046038	1.480951
244.600703	541.215485	18.955290	-0.045992	1.473473
244.543628	533.359724	18.960295	-0.045977	1.465926
244.489083	525.559465	18.965299	-0.045961	1.458394
244.251967	517.780329	18.970304	-0.045912	1.450814
244.568627	509.919937	18.975309	-0.045966	1.443203
244.243371	502.180491	18.980314	-0.045901	1.435568
244.442044	494.332272	18.985319	-0.045932	1.427869
244.463631	486.539688	18.990323	-0.045931	1.420155
244.331687	478.771996	18.995328	-0.045902	1.412398
244.236070	471.007280	19.000333	-0.045879	1.404607
243.733810	463.307710	19.005338	-0.045781	1.396771
243.918105	455.465769	19.010343	-0.045810	1.388861
243.825108	447.693382	19.015347	-0.045787	1.380930
243.807316	439.916515	19.020352	-0.045779	1.372962
243.629917	432.171667	19.025357	-0.045741	1.364952
243.572965	424.408012	19.030362	-0.045725	1.356897
243.598638	416.630636	19.035367	-0.045725	1.348793
243.491587	408.891640	19.040371	-0.045700	1.340658
243.482098	401.130147	19.045376	-0.045694	1.332466
243.397124	393.401107	19.050381	-0.045673	1.324244
243.208061	385.680376	19.055386	-0.045633	1.315962
243.281493	377.790744	19.060391	-0.045641	1.307492
243.062161	370.102630	19.065395	-0.045595	1.299132
242.714610	362.415856	19.070400	-0.045526	1.290696
242.795592	354.682225	19.075405	-0.045536	1.282232
242.733132	346.965381	19.080410	-0.045519	1.273704
242.495178	339.283253	19.085415	-0.045470	1.265124
242.348241	331.592505	19.090419	-0.045437	1.256493
242.403777	323.861096	19.095424	-0.045443	1.247795
242.323649	316.192016	19.100429	-0.045423	1.239080
242.350319	308.466473	19.105434	-0.045423	1.230260
242.276669	300.780456	19.110439	-0.045404	1.221402
242.084409	293.134686	19.115443	-0.045364	1.212503
242.113799	285.433208	19.120448	-0.045364	1.203517
242.100765	277.786552	19.125453	-0.045357	1.194519
242.011264	270.115807	19.130458	-0.045335	1.185409
242.088825	262.453649	19.135463	-0.045345	1.176273
241.709657	254.855527	19.140467	-0.045269	1.167048
241.630948	247.230075	19.145472	-0.045249	1.157779
241.775274	239.534818	19.150477	-0.045271	1.148396
241.438909	231.945576	19.155482	-0.045204	1.138965
241.121611	224.380315	19.160487	-0.045140	1.129490
241.137634	216.747745	19.165491	-0.045138	1.119921
241.130876	209.134239	19.170496	-0.045132	1.110289
240.753092	201.604672	19.175501	-0.045057	1.100599
240.709712	194.005403	19.180506	-0.045044	1.090807
240.653998	186.434397	19.185511	-0.045028	1.080960
240.244410	178.926979	19.190515	-0.044947	1.071025
240.272207	171.328575	19.195520	-0.044947	1.060977
240.556017	163.729730	19.200525	-0.044995	1.050892
240.304652	156.226510	19.205530	-0.044944	1.040714
240.212844	148.713307	19.210535	-0.044922	1.030458
240.289905	141.179136	19.215539	-0.044931	1.020111
239.834719	133.750325	19.220544	-0.044842	1.009677
239.551638	126.311735	19.225549	-0.044784	0.999161
239.195632	118.847505	19.230554	-0.044713	0.988479
239.019671	111.387982	19.235559	-0.044675	0.977731
238.426742	104.016854	19.240563	-0.044560	0.966888
237.779450	96.668294	19.245568	-0.044435	0.955940
237.621439	89.237603	19.250573	-0.044401	0.944870
236.806865	81.935625	19.255578	-0.044244	0.933689
236.347997	74.585849	19.260583	-0.044154	0.922395
235.861094	67.259357	19.265587	-0.044059	0.910989
235.318998	60.170247	19.270592	-0.043953	0.899795