Tue Mar 23 10:54:56 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.605156	0.066355	0.000000	0.000036	0.722169

0.559698	0.191172	0.005005	0.000044	0.722398
0.683833	0.144111	0.010010	0.000021	0.722349
0.108016	0.249235	0.015014	0.000128	0.722354
0.730261	0.073690	0.020019	0.000013	0.722227
0.475269	0.055160	0.025024	0.000060	0.722102
0.485243	0.050994	0.030029	0.000058	0.722097
0.163762	0.116957	0.035034	0.000118	0.722114
0.399727	0.063740	0.040038	0.000074	0.722092
0.542575	0.042910	0.045043	0.000047	0.722101
0.309478	0.087141	0.050048	0.000091	0.722107
0.614650	0.029865	0.055053	0.000034	0.722101
0.532294	0.043526	0.060058	0.000049	0.722099
0.578046	0.032315	0.065062	0.000041	0.722093
0.627126	0.028456	0.070067	0.000031	0.722103
0.281754	0.087471	0.075072	0.000096	0.722098
0.281536	0.088972	0.080077	0.000096	0.722101
0.360166	0.077270	0.085082	0.000081	0.722106
0.166760	0.075431	0.090086	0.000117	0.722035
-0.133532	0.006257	0.095091	0.000173	0.721794
0.166148	-0.057385	0.100096	0.000117	0.721774
0.171541	-0.055177	0.105101	0.000116	0.721780
0.422913	-0.104422	0.110106	0.000069	0.721771
0.466012	-0.119249	0.115110	0.000061	0.721757
0.523313	-0.123344	0.120115	0.000050	0.721769
0.387193	-0.161684	0.125120	0.000076	0.721646
0.372249	-0.252068	0.130125	0.000078	0.721464
0.510806	-0.270790	0.135130	0.000053	0.721475
0.256910	-0.230913	0.140134	0.000100	0.721465
0.353711	-0.249186	0.145139	0.000082	0.721463
0.434221	-0.331107	0.150144	0.000067	0.721330
0.301322	-0.397037	0.155149	0.000091	0.721154
0.322544	-0.399355	0.160154	0.000087	0.721157
0.445329	-0.429950	0.165158	0.000065	0.721140
0.615243	-0.490237	0.170163	0.000033	0.721081
0.483895	-0.563273	0.175168	0.000057	0.720891
0.376373	-0.542352	0.180173	0.000077	0.720895
0.414920	-0.545971	0.185178	0.000070	0.720901
0.353508	-0.645071	0.190182	0.000082	0.720685
0.534816	-0.739317	0.195187	0.000048	0.720563
0.461447	-0.734228	0.200192	0.000061	0.720547
0.419595	-0.776326	0.205197	0.000069	0.720450
0.332627	-0.866964	0.210202	0.000085	0.720241
0.156172	-0.838089	0.215206	0.000118	0.720236
0.500839	-0.924582	0.220211	0.000054	0.720187
0.281814	-1.017924	0.225216	0.000095	0.719926
0.315774	-1.027345	0.230221	0.000088	0.719919
0.398264	-1.088450	0.235226	0.000073	0.719828
0.321604	-1.178970	0.240230	0.000087	0.719623
0.617389	-1.230219	0.245235	0.000032	0.719626
0.511437	-1.329306	0.250240	0.000052	0.719393
0.538531	-1.388823	0.255245	0.000047	0.719285
0.394115	-1.386657	0.260250	0.000074	0.719239
0.035042	-1.456032	0.265254	0.000141	0.718976
-0.196269	-1.401879	0.270259	0.000184	0.719002
-0.101275	-1.519324	0.275264	0.000166	0.718803
-0.765855	-1.456421	0.280269	0.000290	0.718694
-0.877957	-1.429549	0.285274	0.000310	0.718708
-0.233721	-1.688307	0.290278	0.000191	0.718423
-0.109274	-1.725058	0.295283	0.000167	0.718395
-0.005911	-1.834902	0.300288	0.000148	0.718214
-0.088569	-1.906227	0.305293	0.000164	0.718044
-0.180059	-1.925922	0.310298	0.000181	0.717973
-0.770355	-1.937495	0.315302	0.000290	0.717743
-0.238427	-2.038624	0.320307	0.000191	0.717730
-0.485941	-2.158596	0.325312	0.000237	0.717406
-2.336519	-1.832043	0.330317	0.000582	0.717400
-1.946625	-1.959290	0.335322	0.000509	0.717286
-3.144307	-1.843679	0.340326	0.000732	0.717092
-2.600305	-1.935085	0.345331	0.000631	0.717103
-2.771198	-1.974940	0.350336	0.000663	0.716964
-3.778301	-1.894599	0.355341	0.000850	0.716768
-3.600166	-1.925188	0.360346	0.000817	0.716771
-4.142634	-1.837299	0.365350	0.000918	0.716754
-4.195903	-1.970699	0.370355	0.000928	0.716471
-4.681663	-1.885455	0.375360	0.001018	0.716468
-4.840818	-1.860862	0.380365	0.001048	0.716461
-4.406847	-1.996357	0.385370	0.000967	0.716346
-5.674075	-1.872151	0.390374	0.001203	0.716145
-5.493522	-1.897580	0.395379	0.001169	0.716158
-5.657625	-1.874072	0.400384	0.001200	0.716147
-5.694170	-1.896835	0.405389	0.001206	0.716089
-6.331621	-1.880105	0.410394	0.001325	0.715897
-6.096401	-1.924487	0.415398	0.001281	0.715892
-6.017674	-1.934028	0.420403	0.001266	0.715901
-6.398530	-1.867070	0.425408	0.001337	0.715900
-6.916500	-1.918784	0.430413	0.001434	0.715614
-7.181297	-1.887530	0.435418	0.001483	0.715583
-7.825574	-1.773849	0.440422	0.001603	0.715581
-7.283646	-1.875652	0.445427	0.001502	0.715571
-7.451882	-1.843689	0.450432	0.001533	0.715575
-7.537567	-1.939871	0.455437	0.001549	0.715354
-8.415879	-1.833048	0.460442	0.001713	0.715255
-8.380048	-1.843883	0.465446	0.001706	0.715247
-8.115889	-1.882444	0.470451	0.001657	0.715264
-8.510245	-1.820866	0.475456	0.001730	0.715246
-8.417427	-1.845155	0.480461	0.001713	0.715231
-8.580563	-1.970777	0.485466	0.001743	0.714924
-9.465362	-1.817395	0.490470	0.001908	0.714916
-9.171432	-1.869009	0.495475	0.001853	0.714918
-8.750438	-1.947502	0.500480	0.001774	0.714911
-9.007784	-1.901673	0.505485	0.001822	0.714911
-9.151716	-1.926483	0.510490	0.001849	0.714811
-10.050215	-1.866208	0.515494	0.002016	0.714613
-9.369107	-1.981326	0.520499	0.001890	0.714625
-10.111011	-1.852133	0.525504	0.002028	0.714619
-10.400494	-1.800028	0.530509	0.002081	0.714620
-9.887314	-1.890933	0.535514	0.001986	0.714622
-9.943746	-1.925374	0.540518	0.001996	0.714533
-10.990010	-1.857590	0.545523	0.002191	0.714298
-10.998856	-1.856336	0.550528	0.002193	0.714297
-11.224968	-1.816775	0.555533	0.002235	0.714296
-11.048191	-1.842851	0.560538	0.002202	0.714307
-11.017301	-1.858535	0.565542	0.002196	0.714287
-11.030279	-1.852735	0.570547	0.002198	0.714294
-11.166322	-1.894457	0.575552	0.002224	0.714163
-12.230287	-1.799186	0.580557	0.002422	0.713975
-11.570883	-1.910920	0.585562	0.002299	0.713987
-11.886465	-1.861311	0.590566	0.002357	0.713974
-11.901602	-1.857130	0.595571	0.002360	0.713977
-11.682513	-1.892316	0.600576	0.002319	0.713985
-12.044715	-1.832282	0.605581	0.002387	0.713976
-12.002419	-1.937692	0.610586	0.002379	0.713781
-13.171271	-1.793268	0.615590	0.002596	0.713655
-12.539926	-1.899420	0.620595	0.002479	0.713667
-12.576310	-1.895106	0.625600	0.002486	0.713663
-12.953757	-1.826505	0.630605	0.002556	0.713666
-12.555007	-1.892362	0.635610	0.002482	0.713676
-13.174257	-1.783632	0.640614	0.002597	0.713673
-13.017521	-1.913032	0.645619	0.002568	0.713471
-13.679294	-1.845527	0.650624	0.002691	0.713371
-13.611960	-1.859962	0.655629	0.002678	0.713367
-13.548831	-1.863762	0.660634	0.002666	0.713381
-13.949638	-1.800532	0.665638	0.002741	0.713365
-13.517559	-1.871350	0.670643	0.002660	0.713378
-13.817178	-1.814729	0.675648	0.002716	0.713384
-14.138770	-1.879781	0.680653	0.002776	0.713141
-14.640569	-1.837648	0.685658	0.002869	0.713047
-14.553498	-1.862107	0.690662	0.002853	0.713029
-14.489007	-1.868702	0.695667	0.002841	0.713039
-14.770213	-1.818185	0.700672	0.002893	0.713040
-14.428947	-1.881770	0.705677	0.002830	0.713034
-14.215226	-1.917654	0.710682	0.002790	0.713039
-15.246913	-1.855832	0.715686	0.002982	0.712796
-15.852572	-1.775538	0.720691	0.003095	0.712741
-15.855051	-1.780121	0.725696	0.003095	0.712731
-15.811644	-1.789272	0.730701	0.003087	0.712729
-15.530319	-1.835203	0.735706	0.003035	0.712737
-15.611664	-1.826912	0.740710	0.003050	0.712725
-15.603505	-1.826375	0.745715	0.003048	0.712729
-15.896179	-1.772325	0.750720	0.003102	0.712733
-15.908059	-1.914604	0.755725	0.003105	0.712445
-16.612755	-1.810695	0.760730	0.003236	0.712402
-16.907011	-1.761142	0.765734	0.003290	0.712397
-16.214315	-1.876718	0.770739	0.003162	0.712412
-16.307641	-1.867073	0.775744	0.003179	0.712398
-16.724670	-1.794589	0.780749	0.003256	0.712395
-16.370274	-1.847352	0.785754	0.003190	0.712416
-16.435085	-1.930599	0.790758	0.003202	0.712227
-17.862682	-1.734703	0.795763	0.003468	0.712111
-17.164111	-1.859632	0.800768	0.003338	0.712110
-17.059568	-1.880849	0.805773	0.003319	0.712105
-17.304816	-1.832350	0.810778	0.003364	0.712114
-17.629920	-1.781057	0.815782	0.003425	0.712101
-17.425566	-1.813047	0.820787	0.003387	0.712110
-17.247636	-1.942979	0.825792	0.003353	0.711914
-18.738173	-1.746835	0.830797	0.003631	0.711776
-17.940174	-1.889168	0.835802	0.003482	0.711776
-18.347993	-1.820004	0.840806	0.003558	0.711769
-18.730170	-1.746407	0.845811	0.003629	0.711780
-18.498372	-1.785050	0.850816	0.003586	0.711785
-18.437276	-1.798526	0.855821	0.003575	0.711780
-18.740079	-1.730264	0.860826	0.003631	0.711809
-19.012232	-1.846787	0.865830	0.003682	0.711480
-18.982573	-1.852001	0.870835	0.003676	0.711480
-19.439855	-1.768701	0.875840	0.003761	0.711484
-19.246255	-1.809030	0.880845	0.003725	0.711472
-18.960971	-1.854074	0.885850	0.003672	0.711484
-19.192089	-1.821395	0.890854	0.003715	0.711467
-19.096912	-1.832844	0.895859	0.003697	0.711478
-19.829552	-1.847696	0.900864	0.003833	0.711188
-20.118649	-1.816217	0.905869	0.003887	0.711148
-19.697226	-1.890017	0.910874	0.003809	0.711151
-19.870235	-1.861430	0.915878	0.003841	0.711147
-19.874178	-1.854636	0.920883	0.003842	0.711159
-19.877172	-1.857122	0.925888	0.003842	0.711153
-20.141032	-1.840303	0.930893	0.003891	0.711093
-20.890530	-1.804581	0.935898	0.004031	0.710897
-20.645809	-1.856593	0.940902	0.003985	0.710881
-20.594819	-1.862481	0.945907	0.003975	0.710887
-20.739009	-1.836995	0.950912	0.004002	0.710887
-20.621999	-1.860703	0.955917	0.003980	0.710881
-20.465885	-1.886454	0.960922	0.003951	0.710886
-21.070096	-1.893192	0.965926	0.004064	0.710657
-21.858286	-1.807854	0.970931	0.004210	0.710547
-21.337416	-1.899885	0.975936	0.004113	0.710549
-21.729441	-1.833405	0.980941	0.004186	0.710542
-21.906013	-1.797148	0.985946	0.004219	0.710552
-21.381660	-1.896440	0.990950	0.004122	0.710540
-21.620170	-1.850203	0.995955	0.004166	0.710548
-22.400912	-1.838236	1.000960	0.004311	0.710294
-22.884216	-1.783018	1.005965	0.004401	0.710232
-22.192095	-1.902558	1.010970	0.004272	0.710240
-22.514761	-1.850815	1.015974	0.004332	0.710228
-23.004119	-1.761250	1.020979	0.004423	0.710233
-22.642202	-1.827578	1.025984	0.004356	0.710230
-22.863561	-1.783577	1.030989	0.004397	0.710239
-22.629305	-1.899778	1.035994	0.004353	0.710090
-23.777131	-1.786684	1.040998	0.004567	0.709907
-23.441039	-1.845796	1.046003	0.004504	0.709909
-23.730807	-1.793823	1.051008	0.004558	0.709910
-23.846275	-1.775208	1.056013	0.004580	0.709906
-23.165289	-1.894837	1.061018	0.004453	0.709910
-23.789012	-1.785428	1.066022	0.004569	0.709906
-23.989268	-1.748896	1.071027	0.004606	0.709908
-23.730110	-1.945578	1.076032	0.004558	0.709607
-24.334531	-1.836172	1.081037	0.004670	0.709611
-24.791636	-1.749310	1.086042	0.004755	0.709621
-24.468354	-1.811329	1.091046	0.004695	0.709613
-24.285047	-1.842088	1.096051	0.004661	0.709617
-24.428887	-1.818300	1.101056	0.004688	0.709613
-24.891865	-1.734721	1.106061	0.004774	0.709615
-24.909940	-1.873439	1.111066	0.004777	0.709331
-25.740237	-1.740668	1.116070	0.004932	0.709301
-25.753196	-1.745931	1.121075	0.004934	0.709286
-24.938524	-1.893483	1.126080	0.004782	0.709281
-25.426215	-1.811074	1.131085	0.004873	0.709272
-25.653347	-1.764684	1.136090	0.004915	0.709284
-25.334238	-1.826388	1.141094	0.004856	0.709275
-25.107451	-1.955775	1.146099	0.004814	0.709097
-26.172683	-1.829892	1.151104	0.005012	0.708969
-26.186611	-1.828822	1.156109	0.005015	0.708966
-25.869748	-1.883031	1.161114	0.004956	0.708971
-26.162922	-1.835904	1.166118	0.005010	0.708961
-26.285598	-1.807856	1.171123	0.005033	0.708973
-26.027601	-1.858202	1.176128	0.004985	0.708964
-26.827015	-1.870723	1.181133	0.005134	0.708654
-27.143206	-1.814504	1.186138	0.005192	0.708654
-27.262598	-1.798691	1.191142	0.005215	0.708643
-27.095418	-1.826114	1.196147	0.005183	0.708648
-27.113350	-1.823472	1.201152	0.005187	0.708647
-27.378380	-1.777344	1.206157	0.005236	0.708645
-26.761113	-1.885204	1.211162	0.005121	0.708649
-27.312529	-1.905706	1.216166	0.005224	0.708411
-28.237445	-1.766908	1.221171	0.005396	0.708359
-27.896887	-1.829277	1.226176	0.005332	0.708356
-27.816462	-1.841437	1.231181	0.005317	0.708360
-27.743121	-1.851166	1.236186	0.005304	0.708367
-27.919128	-1.823081	1.241190	0.005336	0.708361
-27.784376	-1.843792	1.246195	0.005311	0.708367
-28.571565	-1.870491	1.251200	0.005458	0.708033
-28.875337	-1.818312	1.256205	0.005514	0.708029
-28.780292	-1.833351	1.261210	0.005496	0.708033
-28.742268	-1.848386	1.266214	0.005489	0.708016
-28.859181	-1.825887	1.271219	0.005511	0.708020
-28.813581	-1.832775	1.276224	0.005503	0.708022
-28.546209	-1.895998	1.281229	0.005453	0.707991
-29.383055	-1.885667	1.286234	0.005608	0.707713
-29.717610	-1.829750	1.291238	0.005671	0.707705
-29.708688	-1.829987	1.296243	0.005669	0.707708
-29.604481	-1.845765	1.301248	0.005650	0.707714
-29.755916	-1.821665	1.306253	0.005678	0.707708
-29.761351	-1.813703	1.311258	0.005679	0.707722
-29.670735	-1.847910	1.316262	0.005662	0.707686
-30.199839	-1.900442	1.321267	0.005760	0.707392
-30.720847	-1.804413	1.326272	0.005857	0.707398
-30.973539	-1.765143	1.331277	0.005904	0.707387
-30.459843	-1.852849	1.336282	0.005808	0.707395
-30.738727	-1.807939	1.341286	0.005860	0.707385
-30.297879	-1.885306	1.346291	0.005778	0.707387
-30.579590	-1.836316	1.351296	0.005831	0.707385
-31.512383	-1.811435	1.356301	0.006004	0.707101
-31.568829	-1.803600	1.361306	0.006015	0.707097
-31.472938	-1.823729	1.366310	0.005997	0.707091
-31.632232	-1.792162	1.371315	0.006026	0.707098
-31.790070	-1.768782	1.376320	0.006056	0.707088
-31.689227	-1.786335	1.381325	0.006037	0.707089
-31.371235	-1.834658	1.386330	0.005978	0.707106
-31.821721	-1.813338	1.391334	0.006061	0.706988
-32.560499	-1.792298	1.396339	0.006199	0.706765
-32.008315	-1.892813	1.401344	0.006096	0.706761
-32.702315	-1.771274	1.406349	0.006225	0.706757
-32.255132	-1.843171	1.411354	0.006142	0.706773
-31.987900	-1.897293	1.416358	0.006092	0.706760
-32.702649	-1.768948	1.421363	0.006225	0.706762
-32.540062	-1.856003	1.426368	0.006195	0.706645
-33.223458	-1.830874	1.431373	0.006322	0.706451
-33.121576	-1.844730	1.436378	0.006303	0.706460
-33.655686	-1.748849	1.441382	0.006402	0.706461
-33.438657	-1.782179	1.446387	0.006362	0.706472
-33.225990	-1.820128	1.451392	0.006322	0.706472
-33.978286	-1.686759	1.456397	0.006462	0.706471
-33.640073	-1.739900	1.461402	0.006399	0.706485
-33.603128	-1.894754	1.466406	0.006392	0.706187
-34.214343	-1.806243	1.471411	0.006506	0.706146
-34.237870	-1.805940	1.476416	0.006511	0.706139
-33.909196	-1.865497	1.481421	0.006449	0.706137
-33.909842	-1.860461	1.486426	0.006449	0.706147
-34.343112	-1.787674	1.491430	0.006530	0.706138
-34.141403	-1.847034	1.496435	0.006492	0.706091
-34.822479	-1.828752	1.501440	0.006619	0.705884
-35.068241	-1.792524	1.506445	0.006665	0.705868
-34.840255	-1.830567	1.511450	0.006622	0.705874
-34.667225	-1.865837	1.516454	0.006590	0.705865
-34.754454	-1.847428	1.521459	0.006606	0.705871
-35.013573	-1.800245	1.526464	0.006654	0.705873
-35.001128	-1.903247	1.531469	0.006652	0.705670
-35.747355	-1.836916	1.536474	0.006791	0.705536
-35.941341	-1.801961	1.541478	0.006827	0.705537
-35.828855	-1.820545	1.546483	0.006806	0.705540
-35.652260	-1.851835	1.551488	0.006773	0.705541
-35.934783	-1.803117	1.556493	0.006826	0.705537
-35.695399	-1.845016	1.561498	0.006781	0.705539
-36.252817	-1.883649	1.566502	0.006885	0.705261
-36.718288	-1.823134	1.571507	0.006971	0.705216
-36.692025	-1.824762	1.576512	0.006967	0.705222
-36.681284	-1.827305	1.581517	0.006964	0.705221
-36.450830	-1.866490	1.586522	0.006922	0.705225
-36.674241	-1.830399	1.591526	0.006963	0.705218
-36.517017	-1.871027	1.596531	0.006934	0.705192
-36.914281	-1.945920	1.601536	0.007008	0.704899
-37.357791	-1.868813	1.606541	0.007090	0.704895
-37.714311	-1.800200	1.611546	0.007157	0.704905
-37.412495	-1.858692	1.616550	0.007100	0.704896
-37.386071	-1.857677	1.621555	0.007095	0.704908
-37.512431	-1.836325	1.626560	0.007119	0.704905
-37.876981	-1.835037	1.631565	0.007187	0.704777
-38.154517	-1.870312	1.636570	0.007238	0.704607
-38.415052	-1.828412	1.641574	0.007287	0.704598
-38.636299	-1.786545	1.646579	0.007328	0.704603
-38.509693	-1.803273	1.651584	0.007304	0.704614
-38.545580	-1.799712	1.656589	0.007311	0.704609
-38.726816	-1.763466	1.661594	0.007345	0.704617
-38.593240	-1.804515	1.666598	0.007320	0.704582
-38.888021	-1.905280	1.671603	0.007375	0.704273
-39.317302	-1.822499	1.676608	0.007454	0.704286
-39.827555	-1.737980	1.681613	0.007549	0.704273
-38.663373	-1.944691	1.686618	0.007333	0.704275
-38.985642	-1.893099	1.691622	0.007392	0.704263
-39.539625	-1.791922	1.696627	0.007496	0.704268
-39.057884	-1.934032	1.701632	0.007406	0.704155
-40.236845	-1.826186	1.706637	0.007625	0.703948
-40.100870	-1.845559	1.711642	0.007600	0.703958
-40.162869	-1.835869	1.716646	0.007611	0.703956
-39.996463	-1.863181	1.721651	0.007580	0.703960
-40.179509	-1.824255	1.726656	0.007614	0.703973
-40.518957	-1.769133	1.731661	0.007678	0.703962
-40.032555	-1.917852	1.736666	0.007587	0.703837
-41.139667	-1.818662	1.741670	0.007793	0.703639
-41.024899	-1.838239	1.746675	0.007772	0.703641
-40.804250	-1.876536	1.751680	0.007731	0.703644
-41.134613	-1.821638	1.756685	0.007792	0.703636
-40.935396	-1.854761	1.761690	0.007755	0.703640
-41.164936	-1.813427	1.766694	0.007797	0.703641
-41.104558	-1.887529	1.771699	0.007786	0.703514
-41.947477	-1.819613	1.776704	0.007943	0.703347
-42.124599	-1.790985	1.781709	0.007976	0.703342
-41.870135	-1.832103	1.786714	0.007929	0.703350
-41.666911	-1.868416	1.791718	0.007891	0.703350
-41.890251	-1.831201	1.796723	0.007932	0.703345
-41.673900	-1.870086	1.801728	0.007892	0.703344
-42.039149	-1.900437	1.806733	0.007960	0.703152
-42.963192	-1.802521	1.811738	0.008132	0.703017
-42.861131	-1.821805	1.816742	0.008113	0.703015
-42.491714	-1.891029	1.821747	0.008044	0.703008
-42.812083	-1.826741	1.826752	0.008104	0.703023
-43.167221	-1.766686	1.831757	0.008170	0.703016
-42.734924	-1.844569	1.836762	0.008089	0.703015
-42.705361	-1.918025	1.841766	0.008084	0.702877
-44.131932	-1.752349	1.846771	0.008349	0.702698
-43.473988	-1.868143	1.851776	0.008227	0.702701
-43.864410	-1.803996	1.856781	0.008299	0.702690
-43.763978	-1.813529	1.861786	0.008280	0.702707
-43.545289	-1.858624	1.866790	0.008240	0.702695
-43.634682	-1.841500	1.871795	0.008256	0.702697
-43.521734	-1.922994	1.876800	0.008235	0.702573
-44.964896	-1.765391	1.881805	0.008504	0.702372
-44.290558	-1.883031	1.886810	0.008378	0.702377
-44.417015	-1.864934	1.891814	0.008402	0.702368
-44.563275	-1.835588	1.896819	0.008429	0.702375
-44.283862	-1.885485	1.901824	0.008377	0.702375
-44.592739	-1.834289	1.906829	0.008434	0.702367
-44.624988	-1.910241	1.911834	0.008440	0.702202
-45.519428	-1.815839	1.916838	0.008607	0.702071
-45.498026	-1.814262	1.921843	0.008603	0.702082
-45.515770	-1.809179	1.926848	0.008606	0.702086
-45.695271	-1.781083	1.931853	0.008639	0.702078
-45.195109	-1.865051	1.936858	0.008546	0.702088
-45.114048	-1.885452	1.941862	0.008531	0.702076
-45.697064	-1.868154	1.946867	0.008640	0.701901
-46.764503	-1.744303	1.951872	0.008838	0.701767
-46.336022	-1.827643	1.956877	0.008758	0.701753
-46.324360	-1.827610	1.961882	0.008756	0.701757
-46.665376	-1.765164	1.966886	0.008820	0.701761
-46.454766	-1.805843	1.971891	0.008780	0.701754
-46.288226	-1.828294	1.976896	0.008749	0.701769
-46.539249	-1.790760	1.981901	0.008796	0.701755
-46.785358	-1.888294	1.986906	0.008842	0.701468
-47.454789	-1.775467	1.991910	0.008966	0.701455
-47.680814	-1.741152	1.996915	0.009008	0.701443
-47.054011	-1.849277	2.001920	0.008892	0.701451

-47.732516	-1.723696	2.011917	0.009018	0.701460
-47.221405	-1.821243	2.021914	0.008923	0.701448
-47.622722	-1.838803	2.031910	0.008997	0.701267
-48.180262	-1.806153	2.041907	0.009101	0.701132
-48.004788	-1.750002	2.051904	0.009068	0.701309
-47.681724	-1.749083	2.061901	0.009008	0.701428
-47.468966	-1.772252	2.071898	0.008968	0.701458
-47.426161	-1.784995	2.081894	0.008960	0.701448
-47.244101	-1.817702	2.091891	0.008926	0.701448
-47.217638	-1.823016	2.101888	0.008921	0.701447
-47.472098	-1.774464	2.111885	0.008968	0.701453
-47.380858	-1.794260	2.121882	0.008951	0.701446
-47.335096	-1.803285	2.131878	0.008943	0.701445
-47.269484	-1.815694	2.141875	0.008930	0.701444
-46.933708	-1.744151	2.151872	0.008868	0.701710
-46.663243	-1.768335	2.161869	0.008817	0.701759
-46.330433	-1.831238	2.171866	0.008755	0.701752
-46.533454	-1.795447	2.181862	0.008793	0.701751
-46.221932	-1.786985	2.191859	0.008735	0.701881
-45.286053	-1.855173	2.201856	0.008561	0.702081
-45.371194	-1.840900	2.211853	0.008576	0.702079
-45.444137	-1.828492	2.221850	0.008590	0.702078
-45.460411	-1.824952	2.231846	0.008593	0.702080
-44.818565	-1.799421	2.241843	0.008473	0.702363
-44.849184	-1.784744	2.251840	0.008479	0.702382
-44.368037	-1.871812	2.261837	0.008389	0.702379
-44.625351	-1.819078	2.271834	0.008437	0.702393
-44.100072	-1.761913	2.281830	0.008339	0.702698
-43.549553	-1.859917	2.291827	0.008236	0.702699
-43.801999	-1.816167	2.301824	0.008283	0.702696
-43.449159	-1.829168	2.311821	0.008217	0.702798
-42.904771	-1.819608	2.321818	0.008116	0.703013
-42.739936	-1.847230	2.331814	0.008085	0.703017
-42.835754	-1.833802	2.341811	0.008103	0.703010
-42.466574	-1.799008	2.351808	0.008034	0.703213
-41.797763	-1.851035	2.361805	0.007909	0.703349
-41.998161	-1.815948	2.371802	0.007947	0.703348
-41.828582	-1.847200	2.381798	0.007915	0.703346
-41.300271	-1.808435	2.391795	0.007817	0.703615
-41.154111	-1.822698	2.401792	0.007789	0.703639
-41.018445	-1.843917	2.411789	0.007764	0.703645
-41.102669	-1.765574	2.421786	0.007779	0.703773
-40.347503	-1.806207	2.431782	0.007639	0.703963
-40.386990	-1.801316	2.441779	0.007646	0.703959
-40.291020	-1.806587	2.451776	0.007628	0.703983
-39.490450	-1.809518	2.461773	0.007479	0.704265
-39.306008	-1.842567	2.471770	0.007444	0.704265
-39.252113	-1.853663	2.481766	0.007434	0.704262
-39.104719	-1.799842	2.491763	0.007407	0.704423
-38.455353	-1.831716	2.501760	0.007286	0.704593
-38.328535	-1.851701	2.511757	0.007262	0.704598
-38.402187	-1.840180	2.521754	0.007276	0.704595
-37.849458	-1.810670	2.531750	0.007173	0.704853
-37.575761	-1.839224	2.541747	0.007122	0.704894
-37.476043	-1.853911	2.551744	0.007103	0.704901
-37.442977	-1.807491	2.561741	0.007097	0.705006
-36.717661	-1.829658	2.571738	0.006961	0.705222
-36.782250	-1.818162	2.581734	0.006973	0.705222
-36.750723	-1.823915	2.591731	0.006967	0.705222
-36.314712	-1.762957	2.601728	0.006886	0.705502
-35.978745	-1.800453	2.611725	0.006823	0.705547
-36.097689	-1.781288	2.621722	0.006846	0.705543
-35.321756	-1.813668	2.631718	0.006701	0.705756
-35.017788	-1.810220	2.641715	0.006644	0.705873
-35.003908	-1.810691	2.651712	0.006642	0.705877
-34.842549	-1.842807	2.661709	0.006611	0.705870
-34.307328	-1.806389	2.671706	0.006512	0.706135
-33.970693	-1.864421	2.681702	0.006449	0.706140
-34.360722	-1.796323	2.691699	0.006521	0.706137
-33.800865	-1.808751	2.701696	0.006417	0.706313
-33.318694	-1.820296	2.711693	0.006327	0.706463
-33.348967	-1.818222	2.721690	0.006333	0.706456
-33.169972	-1.839681	2.731686	0.006299	0.706477
-32.649877	-1.793015	2.741683	0.006202	0.706757
-32.226844	-1.866012	2.751680	0.006124	0.706762
-32.363286	-1.840079	2.761677	0.006149	0.706766
-31.941136	-1.826517	2.771674	0.006070	0.706944
-31.627740	-1.808065	2.781670	0.006012	0.707094
-31.585184	-1.817262	2.791667	0.006004	0.707091
-31.278265	-1.861585	2.801664	0.005946	0.707112
-30.963190	-1.777701	2.811661	0.005888	0.707393
-30.578485	-1.846860	2.821658	0.005816	0.707392
-30.539415	-1.857927	2.831654	0.005809	0.707384
-30.374630	-1.793665	2.841651	0.005778	0.707572
-29.577837	-1.868649	2.851648	0.005629	0.707707
-29.664108	-1.853875	2.861645	0.005645	0.707706
-29.461804	-1.887996	2.871642	0.005608	0.707710
-28.940943	-1.837306	2.881638	0.005510	0.707998
-29.092821	-1.796618	2.891635	0.005539	0.708026
-28.766456	-1.854638	2.901632	0.005478	0.708026
-28.630026	-1.799889	2.911629	0.005452	0.708185
-27.617101	-1.892383	2.921626	0.005264	0.708361
-28.162495	-1.796147	2.931622	0.005365	0.708360
-28.052629	-1.816326	2.941619	0.005344	0.708359
-27.327413	-1.805343	2.951616	0.005209	0.708640
-27.006348	-1.857110	2.961613	0.005149	0.708651
-27.070811	-1.845952	2.971610	0.005161	0.708650
-26.948433	-1.787181	2.981606	0.005138	0.708812
-26.235074	-1.839708	2.991603	0.005005	0.708962
-26.388925	-1.808953	3.001600	0.005034	0.708969
-26.420006	-1.773967	3.011597	0.005040	0.709028
-25.366669	-1.838759	3.021594	0.004844	0.709274
-25.615245	-1.794286	3.031590	0.004890	0.709274
-25.346015	-1.842042	3.041587	0.004839	0.709275
-24.922122	-1.795408	3.051584	0.004760	0.709520
-24.644364	-1.802890	3.061581	0.004709	0.709604
-24.480687	-1.830274	3.071578	0.004678	0.709608
-24.587139	-1.771673	3.081574	0.004698	0.709687
-23.783451	-1.809283	3.091571	0.004548	0.709899
-23.809522	-1.805982	3.101568	0.004553	0.709896
-23.731772	-1.819969	3.111565	0.004538	0.709896
-22.811901	-1.828245	3.121562	0.004367	0.710207
-22.999359	-1.787706	3.131558	0.004402	0.710222
-22.771441	-1.829192	3.141555	0.004359	0.710220
-22.578991	-1.803167	3.151552	0.004323	0.710341
-21.663473	-1.867124	3.161549	0.004153	0.710539
-21.779881	-1.847573	3.171546	0.004174	0.710537
-22.035345	-1.802503	3.181542	0.004222	0.710537
-21.209458	-1.821388	3.191539	0.004068	0.710793
-21.180145	-1.784757	3.201536	0.004062	0.710877
-20.945696	-1.826074	3.211533	0.004018	0.710878
-20.901266	-1.802737	3.221530	0.004010	0.710940
-20.492183	-1.773239	3.231526	0.003934	0.711145
-20.042934	-1.854626	3.241523	0.003850	0.711142
-20.426128	-1.786253	3.251520	0.003921	0.711143
-19.421671	-1.815409	3.261517	0.003734	0.711442
-19.055806	-1.871716	3.271514	0.003666	0.711460
-19.407177	-1.808818	3.281510	0.003731	0.711461
-19.318661	-1.769805	3.291507	0.003715	0.711570
-18.513648	-1.812980	3.301504	0.003565	0.711770
-18.426056	-1.825584	3.311501	0.003548	0.711777
-18.511913	-1.813517	3.321498	0.003564	0.711770
-17.760347	-1.785632	3.331494	0.003424	0.712093
-17.719812	-1.787538	3.341491	0.003416	0.712104
-17.775303	-1.779197	3.351488	0.003427	0.712101
-17.045959	-1.817670	3.361485	0.003291	0.712283
-16.826675	-1.801336	3.371482	0.003250	0.712394
-16.791898	-1.807469	3.381478	0.003243	0.712394
-16.672130	-1.811407	3.391475	0.003221	0.712429
-16.003060	-1.787381	3.401472	0.003096	0.712715
-15.773834	-1.827172	3.411469	0.003053	0.712717
-16.067248	-1.772642	3.421466	0.003108	0.712722
-15.310672	-1.797586	3.431462	0.002967	0.712940
-15.053524	-1.800897	3.441459	0.002919	0.713025
-14.903850	-1.824200	3.451456	0.002891	0.713032
-15.002497	-1.772682	3.461453	0.002909	0.713100
-13.992023	-1.817967	3.471450	0.002721	0.713368
-14.181868	-1.785618	3.481446	0.002756	0.713365
-14.109940	-1.799115	3.491443	0.002743	0.713364
-13.700720	-1.777198	3.501440	0.002667	0.713553
-13.024308	-1.845094	3.511437	0.002541	0.713658
-13.301585	-1.794854	3.521434	0.002592	0.713660
-13.188849	-1.798605	3.531430	0.002571	0.713692
-12.524990	-1.774631	3.541427	0.002447	0.713975
-12.174170	-1.837334	3.551424	0.002382	0.713975
-12.295955	-1.814753	3.561421	0.002404	0.713977
-12.096156	-1.754186	3.571418	0.002367	0.714168
-11.403516	-1.820869	3.581414	0.002238	0.714281
-11.590599	-1.786380	3.591411	0.002273	0.714284
-11.376493	-1.802154	3.601408	0.002233	0.714328
-10.529089	-1.807902	3.611405	0.002075	0.714617
-10.537230	-1.805799	3.621402	0.002076	0.714619
-10.242293	-1.857798	3.631398	0.002021	0.714620
-10.532465	-1.742100	3.641395	0.002075	0.714747
-9.461485	-1.846870	3.651392	0.001876	0.714918
-9.475134	-1.845596	3.661389	0.001878	0.714916
-9.385977	-1.861531	3.671386	0.001862	0.714916
-8.618199	-1.880689	3.681382	0.001718	0.715150
-8.634684	-1.834723	3.691379	0.001721	0.715235
-8.439682	-1.866556	3.701376	0.001685	0.715241
-8.228241	-1.904310	3.711373	0.001646	0.715241
-7.802003	-1.872703	3.721370	0.001566	0.715455
-7.521131	-1.872153	3.731366	0.001514	0.715555
-7.497947	-1.879016	3.741363	0.001509	0.715550
-7.433353	-1.890773	3.751360	0.001497	0.715550
-6.558596	-1.912431	3.761357	0.001334	0.715816
-6.591258	-1.870125	3.771354	0.001340	0.715888
-6.121497	-1.954437	3.781350	0.001253	0.715887
-6.476338	-1.891491	3.791347	0.001319	0.715887
-6.029023	-1.880804	3.801344	0.001235	0.716066
-5.702331	-1.902604	3.811341	0.001174	0.716138
-5.846500	-1.878205	3.821338	0.001201	0.716136
-5.574924	-1.899415	3.831334	0.001150	0.716190
-4.896028	-1.886136	3.841331	0.001024	0.716456
-4.779704	-1.904067	3.851328	0.001002	0.716462
-4.965734	-1.870083	3.861325	0.001037	0.716464
-4.245478	-1.884205	3.871322	0.000902	0.716690
-3.924298	-1.901199	3.881318	0.000842	0.716770
-4.183118	-1.858436	3.891315	0.000891	0.716763
-3.670328	-1.926208	3.901312	0.000795	0.716810
-3.206464	-1.864437	3.911309	0.000709	0.717096
-2.855860	-1.924797	3.921306	0.000643	0.717100
-3.124766	-1.878385	3.931302	0.000693	0.717098
-2.797053	-1.843071	3.941299	0.000632	0.717283
-2.167414	-1.900656	3.951296	0.000515	0.717391
-2.410290	-1.858051	3.961293	0.000560	0.717390
-2.054281	-1.888750	3.971290	0.000493	0.717455
-1.902838	-1.785868	3.981286	0.000465	0.717712
-1.568368	-1.846909	3.991283	0.000403	0.717709
-1.409296	-1.867820	4.001280	0.000373	0.717724
-1.219348	-1.745486	4.011277	0.000337	0.718033
-1.265326	-1.738737	4.021274	0.000346	0.718030
-1.240558	-1.699896	4.031270	0.000341	0.718116
-1.083456	-1.603952	4.041267	0.000312	0.718361
-1.330084	-1.558625	4.051264	0.000358	0.718364
-0.869117	-1.494740	4.061261	0.000272	0.718652
-0.947422	-1.476062	4.071258	0.000286	0.718662
-0.770575	-1.370906	4.081254	0.000253	0.718932
-0.956555	-1.312818	4.091251	0.000287	0.718981
-1.135974	-1.124039	4.101248	0.000321	0.719291
-0.774231	-1.136803	4.111245	0.000253	0.719393
-0.925803	-0.993045	4.121242	0.000281	0.719623
-0.727391	-0.921002	4.131238	0.000244	0.719835
-0.605350	-0.861701	4.141235	0.000221	0.719995
-0.573324	-0.743038	4.151232	0.000215	0.720240
-0.412138	-0.641058	4.161229	0.000185	0.720498
-0.216221	-0.573439	4.171226	0.000148	0.720700
-0.087727	-0.495930	4.181222	0.000124	0.720898
-0.251054	-0.346221	4.191219	0.000154	0.721135
-0.148162	-0.243234	4.201216	0.000135	0.721374
-0.044852	-0.139605	4.211213	0.000116	0.721614
-0.259025	0.033827	4.221210	0.000155	0.721881
0.009441	0.131050	4.231206	0.000105	0.722166
0.000000	0.303664	4.241203	0.000107	0.722502

0.153459	0.909514	4.246208	0.000078	0.723744
0.413171	2.132942	4.251213	0.000029	0.726229
0.446169	3.984254	4.256218	0.000021	0.729849
1.064672	6.289127	4.261222	-0.000096	0.734528
1.362770	9.154181	4.266227	-0.000153	0.740144
1.875651	12.473011	4.271232	-0.000251	0.746652
2.339912	16.256734	4.276237	-0.000340	0.753963
2.852131	20.434760	4.281242	-0.000438	0.761954
3.219408	25.045033	4.286246	-0.000509	0.770611
3.462401	30.035030	4.291251	-0.000558	0.779822
4.026984	35.318068	4.296256	-0.000666	0.789555
4.641479	40.912458	4.301261	-0.000784	0.799738
5.047938	46.843176	4.306266	-0.000864	0.810317
5.490835	53.057594	4.311270	-0.000951	0.821260
5.925562	59.543247	4.316275	-0.001036	0.832519
6.232219	66.271690	4.321280	-0.001097	0.843998
9.195436	72.762049	4.326285	-0.001653	0.855704
10.518663	79.783626	4.331290	-0.001904	0.867647
11.523854	87.061248	4.336294	-0.002096	0.879750
12.393576	94.533546	4.341299	-0.002263	0.891960
12.879544	102.232608	4.346304	-0.002359	0.904254
13.854552	109.998347	4.351309	-0.002545	0.916620
14.497129	117.928741	4.356314	-0.002670	0.928982
15.599225	125.911642	4.361318	-0.002881	0.941382
16.484809	134.040966	4.366323	-0.003051	0.953781
17.007410	142.307844	4.371328	-0.003154	0.966130
17.529029	150.650007	4.376333	-0.003256	0.978432
18.480483	158.984956	4.381338	-0.003439	0.990677
19.331405	167.396772	4.386342	-0.003603	1.002856
20.093490	175.864065	4.391347	-0.003750	1.014944
21.044178	184.335490	4.396352	-0.003933	1.026941
21.852316	192.881476	4.401357	-0.004089	1.038866
22.511079	201.472988	4.406362	-0.004217	1.050683
23.128447	210.104269	4.411366	-0.004338	1.062410
23.953102	218.718708	4.416371	-0.004497	1.074035
25.115840	227.270614	4.421376	-0.004719	1.085529
25.920947	235.909788	4.426381	-0.004875	1.096935
26.421906	244.603578	4.431386	-0.004974	1.108227
27.633177	253.186261	4.436390	-0.005205	1.119417
28.532818	261.814923	4.441395	-0.005378	1.130487
29.139661	270.492041	4.446400	-0.005497	1.141448
29.920801	279.177513	4.451405	-0.005648	1.152350
30.853731	287.773185	4.456410	-0.005828	1.163072
31.538023	296.414544	4.461414	-0.005961	1.173700
31.945368	305.077794	4.466419	-0.006042	1.184201
32.703705	313.676778	4.471424	-0.006189	1.194605
33.326063	322.275265	4.476429	-0.006311	1.204890
33.894907	330.879001	4.481434	-0.006422	1.215084
34.479247	339.471432	4.486438	-0.006537	1.225183
35.168870	348.049330	4.491443	-0.006671	1.235202
35.852488	356.572469	4.496448	-0.006804	1.245077
36.481061	365.118036	4.501453	-0.006926	1.254889
37.115504	373.626704	4.506458	-0.007050	1.264584
37.744608	382.147644	4.511462	-0.007173	1.274218
38.621431	390.586096	4.516467	-0.007342	1.283734
39.316421	399.078232	4.521472	-0.007477	1.293205
39.679770	407.600642	4.526477	-0.007550	1.302579
40.101838	416.162286	4.531482	-0.007634	1.311939
40.841084	424.627877	4.536486	-0.007777	1.321187
41.413800	433.046679	4.541491	-0.007889	1.330290
41.877180	441.475133	4.546496	-0.007981	1.339322
42.815960	449.826307	4.551501	-0.008162	1.348295
43.428561	458.221432	4.556506	-0.008281	1.357198
43.878097	466.619103	4.561510	-0.008370	1.366017
44.593587	474.987795	4.566515	-0.008509	1.374795
44.921602	483.381040	4.571520	-0.008576	1.383476
45.480053	491.768068	4.576525	-0.008685	1.392136
45.999225	500.111540	4.581530	-0.008787	1.400691
46.956761	508.389325	4.586534	-0.008971	1.409201
47.437070	516.759074	4.591539	-0.009066	1.417672
47.854718	525.105188	4.596544	-0.009149	1.426059
48.462696	533.443833	4.601549	-0.009268	1.434421
49.046426	541.744526	4.606554	-0.009382	1.442692
49.416199	550.090579	4.611558	-0.009456	1.450927
49.898092	558.395502	4.616563	-0.009552	1.459092
50.501975	566.683064	4.621568	-0.009670	1.467214
51.087356	575.040789	4.626573	-0.009784	1.475356
51.344221	583.334581	4.631578	-0.009837	1.483341
52.044139	591.580369	4.636582	-0.009973	1.491306
52.578287	599.856497	4.641587	-0.010078	1.499231
52.802116	608.153888	4.646592	-0.010125	1.507087
53.170083	616.457448	4.651597	-0.010199	1.514930
53.795001	624.673715	4.656602	-0.010321	1.522690
54.283251	632.926615	4.661606	-0.010417	1.530423
54.521932	641.230396	4.666611	-0.010467	1.538127
55.183108	649.432789	4.671616	-0.010596	1.545763
56.014861	657.658765	4.676621	-0.010756	1.553407
56.332698	665.904993	4.681626	-0.010820	1.560957
56.729157	674.153843	4.686630	-0.010900	1.568484
57.316210	682.370627	4.691635	-0.011014	1.575974
57.603779	690.621390	4.696640	-0.011073	1.583415
58.298508	698.823981	4.701645	-0.011208	1.590837
58.651441	707.054425	4.706650	-0.011279	1.598200
58.953708	715.288960	4.711654	-0.011341	1.605525
59.333630	723.526676	4.716659	-0.011417	1.612831
59.758763	731.735199	4.721664	-0.011502	1.620085
60.310096	739.929320	4.726669	-0.011610	1.627311
60.711445	748.195639	4.731674	-0.011690	1.634547
61.094828	756.383642	4.736678	-0.011767	1.641681
61.512636	764.572640	4.741683	-0.011850	1.648789
61.752724	772.785052	4.746688	-0.011900	1.655863
62.380203	780.936562	4.751693	-0.012022	1.662907
63.034333	789.074969	4.756698	-0.012149	1.669913
63.486834	797.284492	4.761702	-0.012239	1.676923
63.801226	805.480416	4.766707	-0.012303	1.683874
64.357068	813.644491	4.771712	-0.012412	1.690801
64.834717	821.835746	4.776717	-0.012506	1.697712
65.202418	830.010627	4.781722	-0.012580	1.704568
65.595346	838.225057	4.786726	-0.012658	1.711431
65.904535	846.421694	4.791731	-0.012721	1.718242
66.065206	854.597533	4.796736	-0.012757	1.724989
66.233252	862.816457	4.801741	-0.012793	1.731746
66.511597	870.978001	4.806746	-0.012851	1.738444
66.942901	879.118765	4.811750	-0.012936	1.745119
67.214584	887.310694	4.816755	-0.012992	1.751789
68.059423	895.399017	4.821760	-0.013155	1.758423
68.634295	903.518991	4.826765	-0.013267	1.765023
68.948586	911.693128	4.831770	-0.013331	1.771609
69.306811	919.873172	4.836774	-0.013403	1.778181
69.826422	927.990169	4.841779	-0.013505	1.784699
70.237377	936.181461	4.846784	-0.013587	1.791237
70.893445	944.331298	4.851789	-0.013715	1.797750
71.382596	952.428773	4.856794	-0.013811	1.804177
71.902025	960.562324	4.861798	-0.013913	1.810613
72.181041	968.745387	4.866803	-0.013971	1.817035
72.736427	976.850828	4.871808	-0.014079	1.823408
73.433228	984.979569	4.876813	-0.014214	1.829793
73.491739	993.176119	4.881818	-0.014231	1.836133
73.849299	1001.321501	4.886822	-0.014303	1.842447
74.228587	1009.464141	4.891827	-0.014379	1.848739
74.500113	1017.618264	4.896832	-0.014435	1.855006
74.521625	1025.807255	4.901837	-0.014444	1.861250
74.867842	1033.920518	4.906842	-0.014514	1.867452
75.342489	1042.069824	4.911846	-0.014607	1.873676
75.715490	1050.176570	4.916851	-0.014682	1.879836
75.948780	1058.296992	4.921856	-0.014731	1.885969
76.642369	1066.396953	4.926861	-0.014866	1.892120
76.862920	1074.541636	4.931866	-0.014912	1.898230
77.132964	1082.668556	4.936870	-0.014968	1.904314
77.514833	1090.792394	4.941875	-0.015044	1.910387
77.882105	1098.913596	4.946880	-0.015118	1.916438
78.269254	1107.033231	4.951885	-0.015195	1.922471
78.386119	1115.181808	4.956890	-0.015222	1.928476
78.884772	1123.300410	4.961894	-0.015320	1.934483
79.242646	1131.404878	4.966899	-0.015392	1.940445
79.314942	1139.551048	4.971904	-0.015411	1.946388
80.012134	1147.674869	4.976909	-0.015546	1.952364
80.311640	1155.793669	4.981914	-0.015608	1.958276
80.531505	1163.902403	4.986918	-0.015654	1.964153
81.097989	1171.965890	4.991923	-0.015765	1.970018
81.513536	1180.063326	4.996928	-0.015847	1.975873
82.038073	1188.152111	5.001933	-0.015950	1.981717
82.061855	1196.298671	5.006938	-0.015960	1.987531
82.430815	1204.422515	5.011942	-0.016034	1.993348
82.806123	1212.519664	5.016947	-0.016109	1.999130
82.839403	1220.630422	5.021952	-0.016121	2.004869
83.420671	1228.723373	5.026957	-0.016234	2.010637
83.823572	1236.813031	5.031962	-0.016315	2.016366
84.080272	1244.932889	5.036966	-0.016368	2.022086
84.255678	1253.068035	5.041971	-0.016406	2.027792
84.605433	1261.192328	5.046976	-0.016476	2.033491
84.929323	1269.297874	5.051981	-0.016542	2.039160
85.097186	1277.370892	5.056986	-0.016579	2.044774
85.585769	1285.462246	5.061990	-0.016675	2.050417
85.832417	1293.570646	5.066995	-0.016726	2.056033
85.737439	1301.704942	5.072000	-0.016714	2.061616
86.251568	1309.779017	5.077005	-0.016815	2.067204
86.650800	1317.861699	5.082010	-0.016895	2.072771
86.828562	1325.984217	5.087014	-0.016933	2.078329
87.530764	1334.001452	5.092019	-0.017069	2.083852
87.827439	1342.109249	5.097024	-0.017130	2.089381
88.395475	1350.191385	5.102029	-0.017241	2.094905
88.563646	1358.292235	5.107034	-0.017277	2.100388
88.931769	1366.383894	5.112038	-0.017351	2.105870
89.124576	1374.556690	5.117043	-0.017392	2.111375
89.585539	1382.642790	5.122048	-0.017484	2.116834
89.930388	1390.724005	5.127053	-0.017553	2.122264
89.963139	1398.823164	5.132058	-0.017565	2.127662
90.299722	1406.921461	5.137062	-0.017633	2.133075
90.596426	1414.993014	5.142067	-0.017693	2.138452
90.959324	1423.042792	5.147072	-0.017766	2.143808
91.242948	1431.161292	5.152077	-0.017824	2.149188
91.253627	1439.288693	5.157082	-0.017831	2.154535
91.820003	1447.319265	5.162086	-0.017942	2.159857
92.109721	1455.397743	5.167091	-0.018001	2.165172
92.089513	1463.515198	5.172096	-0.018003	2.170470
92.749357	1471.587203	5.177101	-0.018131	2.175788
92.940895	1479.658732	5.182106	-0.018172	2.181050
93.022052	1487.773483	5.187110	-0.018193	2.186317
93.395113	1495.864946	5.192115	-0.018267	2.191583
93.742853	1503.934423	5.197120	-0.018337	2.196819
94.185743	1511.981846	5.202125	-0.018425	2.202038
94.429948	1520.052792	5.207130	-0.018476	2.207241
94.637395	1528.157657	5.212134	-0.018520	2.212451
95.101700	1536.217137	5.217139	-0.018612	2.217642
95.161034	1544.303797	5.222144	-0.018628	2.222802
95.349219	1552.414379	5.227149	-0.018668	2.227976
95.709094	1560.485745	5.232154	-0.018741	2.233129
96.021086	1568.566414	5.237158	-0.018804	2.238272
96.458916	1576.601854	5.242163	-0.018891	2.243386
96.944638	1584.644332	5.247168	-0.018987	2.248496
97.380789	1592.738453	5.252173	-0.019073	2.253622
97.392479	1600.836957	5.257178	-0.019081	2.258703
97.609831	1608.935719	5.262182	-0.019127	2.263790
97.811311	1617.027782	5.267187	-0.019169	2.268861
98.290424	1625.137885	5.272192	-0.019264	2.273955
98.462885	1633.229376	5.277197	-0.019301	2.278999
98.860244	1641.238924	5.282202	-0.019381	2.284001
99.699730	1649.222939	5.287206	-0.019542	2.289014
100.120909	1657.317168	5.292211	-0.019626	2.294048
100.081448	1665.418846	5.297216	-0.019624	2.299037
100.647428	1673.463338	5.302221	-0.019735	2.304030
100.673199	1681.562107	5.307226	-0.019745	2.309001
101.094153	1689.643548	5.312230	-0.019828	2.313984
101.506346	1697.685321	5.317235	-0.019910	2.318930
101.734812	1705.744963	5.322240	-0.019958	2.323862
102.063645	1713.834455	5.327245	-0.020025	2.328809
102.297334	1721.917745	5.332250	-0.020074	2.333735
102.620104	1729.980408	5.337254	-0.020139	2.338645
103.103548	1738.029969	5.342259	-0.020234	2.343549
103.247217	1746.125035	5.347264	-0.020266	2.348443
103.790262	1754.212280	5.352269	-0.020373	2.353355
103.729925	1762.310950	5.357274	-0.020367	2.358214
103.888523	1770.375719	5.362278	-0.020402	2.363061
104.377786	1778.394448	5.367283	-0.020498	2.367896
104.661305	1786.471909	5.372288	-0.020556	2.372741
105.539585	1794.483780	5.377293	-0.020725	2.377583
105.921445	1802.535355	5.382298	-0.020802	2.382400
106.265953	1810.599789	5.387302	-0.020871	2.387212
106.223495	1818.730760	5.392307	-0.020868	2.392023
106.529245	1826.785433	5.397312	-0.020931	2.396806
107.004886	1834.826399	5.402317	-0.021025	2.401585
107.291424	1842.875628	5.407322	-0.021083	2.406344
107.775838	1850.938435	5.412326	-0.021179	2.411118
108.238935	1859.013442	5.417331	-0.021270	2.415887
108.559503	1867.063466	5.422336	-0.021335	2.420621
108.867913	1875.139907	5.427341	-0.021398	2.425361
109.126865	1883.213670	5.432346	-0.021451	2.430085
109.373102	1891.371898	5.437350	-0.021503	2.434849
109.643305	1899.404762	5.442355	-0.021558	2.439532
109.687621	1907.446203	5.447360	-0.021572	2.444194
110.006337	1915.510596	5.452365	-0.021636	2.448882
110.226525	1923.574033	5.457370	-0.021683	2.453552
110.599461	1931.609708	5.462374	-0.021757	2.458208
110.839166	1939.667646	5.467379	-0.021807	2.462859
110.733720	1947.766862	5.472384	-0.021793	2.467499
110.984676	1955.843931	5.477389	-0.021845	2.472144
111.081074	1963.908050	5.482394	-0.021868	2.476761
111.676314	1971.878817	5.487398	-0.021984	2.481353
112.076702	1979.932478	5.492403	-0.022064	2.485970
111.989052	1988.035309	5.497408	-0.022053	2.490570
112.342844	1996.108231	5.502413	-0.022125	2.495177
112.720259	2004.108575	5.507418	-0.022200	2.499736
113.124147	2012.135289	5.512422	-0.022281	2.504303
113.643749	2020.189470	5.517427	-0.022383	2.508886
113.732739	2028.330302	5.522432	-0.022405	2.513478
113.814140	2036.420090	5.527437	-0.022425	2.518032
114.179903	2044.407498	5.532442	-0.022498	2.522541
114.630478	2052.426218	5.537446	-0.022588	2.527066
114.660674	2060.546147	5.542451	-0.022598	2.531609
114.734088	2068.623970	5.547456	-0.022617	2.536123
115.276508	2076.637024	5.552461	-0.022724	2.540627
115.595735	2084.667675	5.557466	-0.022788	2.545116
115.872456	2092.750739	5.562470	-0.022845	2.549624
116.031615	2100.840041	5.567475	-0.022880	2.554118
116.343052	2108.847383	5.572480	-0.022944	2.558571
116.534602	2116.922740	5.577485	-0.022985	2.563044
116.787974	2124.977348	5.582490	-0.023037	2.567503
117.054759	2133.039894	5.587494	-0.023092	2.571959
117.254811	2141.111321	5.592499	-0.023135	2.576407
117.304645	2149.166941	5.597504	-0.023149	2.580829
117.749784	2157.182117	5.602509	-0.023237	2.585248
117.860895	2165.253006	5.607514	-0.023263	2.589667
117.977330	2173.512894	5.612518	-0.023290	2.594182
118.305653	2181.504748	5.617523	-0.023357	2.598558
118.794605	2189.431130	5.622528	-0.023453	2.602902
119.160690	2197.449901	5.627533	-0.023526	2.607280
119.206520	2205.534168	5.632538	-0.023540	2.611664
119.507300	2213.569622	5.637542	-0.023602	2.616032
119.551901	2221.634717	5.642547	-0.023615	2.620391
119.684869	2229.654580	5.647552	-0.023645	2.624725
120.127031	2237.670611	5.652557	-0.023733	2.629070
120.507860	2245.724866	5.657562	-0.023809	2.633424
120.597165	2253.794399	5.662566	-0.023831	2.637760
120.895695	2261.847845	5.667571	-0.023892	2.642094
121.194818	2269.840138	5.672576	-0.023953	2.646388
121.476359	2277.904508	5.677581	-0.024011	2.650712
121.613505	2285.973454	5.682586	-0.024041	2.655022
121.769151	2294.041022	5.687590	-0.024076	2.659326
122.247100	2302.060827	5.692595	-0.024170	2.663618
122.510090	2310.095795	5.697600	-0.024224	2.667897
123.041661	2318.162025	5.702605	-0.024329	2.672204
123.456428	2326.213172	5.707610	-0.024411	2.676487
123.421477	2334.259569	5.712614	-0.024410	2.680733
123.776777	2342.298338	5.717619	-0.024481	2.684993
124.021771	2350.325367	5.722624	-0.024532	2.689232
124.499304	2358.389009	5.727629	-0.024626	2.693499
124.615147	2366.447768	5.732634	-0.024653	2.697734
124.733930	2374.497436	5.737638	-0.024681	2.701957
125.045856	2382.533097	5.742643	-0.024744	2.706179
125.064805	2390.591935	5.747648	-0.024753	2.710387
125.474243	2398.653342	5.752653	-0.024834	2.714615
125.870478	2406.658297	5.757658	-0.024913	2.718806
125.943833	2414.715398	5.762662	-0.024932	2.722998
126.325436	2422.773098	5.767667	-0.025009	2.727202
126.432177	2430.816296	5.772672	-0.025034	2.731376
127.884394	2438.763578	5.777677	-0.025310	2.735576
128.725147	2446.776713	5.782682	-0.025471	2.739765
129.223313	2454.821149	5.787686	-0.025569	2.743944
129.442967	2462.943664	5.792691	-0.025616	2.748139
129.388309	2471.070209	5.797696	-0.025611	2.752313
129.937543	2479.161424	5.802701	-0.025718	2.756500
130.432350	2487.139955	5.807706	-0.025816	2.760619
130.492040	2495.152821	5.812710	-0.025832	2.764723
130.522610	2503.240951	5.817715	-0.025843	2.768858
130.780710	2511.288378	5.822720	-0.025897	2.772979
131.220706	2519.316981	5.827725	-0.025984	2.777095
131.310887	2527.368245	5.832730	-0.026006	2.781196
131.572397	2535.377164	5.837734	-0.026060	2.785280
131.897861	2543.437411	5.842739	-0.026126	2.789387
132.069190	2551.500379	5.847744	-0.026163	2.793481
132.430666	2559.526185	5.852749	-0.026236	2.797561
132.776540	2567.537253	5.857754	-0.026305	2.801626
132.966277	2575.569414	5.862758	-0.026346	2.805687
133.120449	2583.646569	5.867763	-0.026380	2.809763
133.477709	2591.694283	5.872768	-0.026452	2.813830
133.698940	2599.743874	5.877773	-0.026498	2.817884
133.783537	2607.792728	5.882778	-0.026519	2.821924
133.808226	2615.858119	5.887782	-0.026529	2.825962
134.249225	2623.877128	5.892787	-0.026616	2.829996
134.206814	2631.973946	5.897792	-0.026614	2.834035
134.513866	2639.991322	5.902797	-0.026676	2.838049
134.904908	2647.983111	5.907802	-0.026754	2.842049
135.118931	2656.018935	5.912806	-0.026800	2.846055
135.377196	2664.056815	5.917811	-0.026853	2.850059
135.589780	2672.114440	5.922816	-0.026898	2.854065
135.901345	2680.159771	5.927821	-0.026961	2.858064
135.909141	2688.201294	5.932826	-0.026968	2.862039
136.157464	2696.223931	5.937830	-0.027019	2.866012
136.466677	2704.282739	5.942835	-0.027082	2.870001
136.730535	2712.320542	5.947840	-0.027137	2.873972
136.860775	2720.367958	5.952845	-0.027166	2.877934
137.122103	2728.376336	5.957850	-0.027220	2.881879
137.107884	2736.431495	5.962854	-0.027223	2.885827
137.376623	2744.489335	5.967859	-0.027278	2.889785
137.534629	2752.534186	5.972864	-0.027313	2.893726
137.989798	2760.550276	5.977869	-0.027403	2.897664
138.235314	2768.585229	5.982874	-0.027454	2.901594
138.284002	2776.642584	5.987878	-0.027468	2.905519
138.796855	2784.667650	5.992883	-0.027569	2.909447
139.050422	2792.790165	5.997888	-0.027622	2.913404
139.178449	2800.844801	6.002893	-0.027651	2.917316
139.439776	2808.823511	6.007898	-0.027705	2.921193
139.691342	2816.817908	6.012902	-0.027757	2.925072
139.900592	2824.881359	6.017907	-0.027801	2.928976
139.875759	2832.948707	6.022912	-0.027802	2.932865
140.538600	2840.935384	6.027917	-0.027930	2.936746
140.630824	2848.975864	6.032922	-0.027953	2.940618
140.739971	2856.982895	6.037926	-0.027978	2.944470
141.174026	2865.035802	6.042931	-0.028064	2.948355
141.286351	2873.104179	6.047936	-0.028091	2.952226
141.396474	2881.184104	6.052941	-0.028117	2.956098
141.974361	2889.138904	6.057946	-0.028229	2.959928
142.181004	2897.172187	6.062950	-0.028273	2.963772
142.338037	2905.206891	6.067955	-0.028308	2.967609
142.515275	2913.254526	6.072960	-0.028346	2.971448
142.874156	2921.314380	6.077965	-0.028418	2.975297
143.027387	2929.346161	6.082970	-0.028452	2.979117
143.075615	2937.392879	6.087974	-0.028466	2.982935
143.323752	2945.427470	6.092979	-0.028518	2.986751
143.432344	2953.450877	6.097984	-0.028543	2.990551
143.748604	2961.554612	6.102989	-0.028607	2.994394
143.946511	2969.550239	6.107994	-0.028649	2.998175
144.207085	2977.553469	6.112998	-0.028703	3.001958
144.595907	2985.576739	6.118003	-0.028781	3.005751
144.904432	2993.570222	6.123008	-0.028844	3.009523
145.119738	3001.662187	6.128013	-0.028889	3.013330
145.270517	3009.717243	6.133018	-0.028922	3.017113
145.338264	3017.767105	6.138022	-0.028940	3.020884
145.625372	3025.794272	6.143027	-0.028999	3.024651
145.943255	3033.800983	6.148032	-0.029064	3.028405
145.974718	3041.888289	6.153037	-0.029075	3.032178
146.182559	3049.931265	6.158042	-0.029119	3.035934
146.420583	3057.898606	6.163046	-0.029168	3.039652
146.740066	3065.946123	6.168051	-0.029233	3.043406
146.788209	3073.979765	6.173056	-0.029247	3.047136
147.143179	3082.041728	6.178061	-0.029319	3.050889
147.264412	3090.091145	6.183066	-0.029347	3.054621
147.582570	3098.120242	6.188070	-0.029411	3.058348
147.734279	3106.156642	6.193075	-0.029445	3.062066
147.877129	3114.163831	6.198080	-0.029477	3.065766
147.999943	3122.218071	6.203085	-0.029505	3.069482
148.211666	3130.308447	6.208090	-0.029549	3.073214
148.483881	3138.335357	6.213094	-0.029605	3.076915
148.705365	3146.354054	6.218099	-0.029652	3.080605
148.631275	3154.355005	6.223104	-0.029643	3.084270
149.067313	3162.346928	6.228109	-0.029730	3.087949
149.193020	3170.409110	6.233114	-0.029759	3.091641
149.318783	3178.455692	6.238118	-0.029787	3.095323
149.913482	3186.460973	6.243123	-0.029903	3.099002
150.003772	3194.477694	6.248128	-0.029925	3.102659
150.106003	3202.529506	6.253133	-0.029950	3.106328
150.445714	3210.553572	6.258138	-0.030018	3.109991
150.674079	3218.601067	6.263142	-0.030066	3.113656
150.867311	3226.663706	6.268147	-0.030107	3.117321
151.038949	3234.657388	6.273152	-0.030144	3.120950
151.147469	3242.682566	6.278157	-0.030170	3.124585
151.491808	3250.716777	6.283162	-0.030239	3.128232
151.502228	3258.779470	6.288166	-0.030247	3.131872
151.692696	3266.834616	6.293171	-0.030287	3.135512
151.992621	3274.822633	6.298176	-0.030348	3.139122
152.271704	3282.863011	6.303181	-0.030406	3.142751
152.285162	3290.907401	6.308186	-0.030414	3.146366
152.463443	3298.911634	6.313190	-0.030452	3.149966
152.882505	3306.993066	6.318195	-0.030535	3.153607
153.011601	3315.022810	6.323200	-0.030565	3.157208
153.122219	3323.039830	6.328205	-0.030591	3.160799
153.323555	3331.044001	6.333210	-0.030633	3.164383
153.459889	3339.067806	6.338214	-0.030664	3.167969
153.721545	3347.151128	6.343219	-0.030718	3.171583
153.890085	3355.165021	6.348224	-0.030755	3.175158
154.072249	3363.201486	6.353229	-0.030794	3.178740
153.961965	3371.255316	6.358234	-0.030779	3.182313
154.322290	3379.243082	6.363238	-0.030851	3.185872
154.631180	3387.277981	6.368243	-0.030914	3.189446
154.719966	3395.309048	6.373248	-0.030936	3.193005
154.823211	3403.392970	6.378253	-0.030960	3.196584
155.001302	3411.384180	6.383258	-0.030999	3.200121
155.156377	3419.394284	6.388262	-0.031033	3.203662
155.797255	3427.394600	6.393267	-0.031157	3.207215
155.844796	3435.435646	6.398272	-0.031171	3.210757
156.133561	3443.505642	6.403277	-0.031231	3.214317
156.485631	3451.524066	6.408282	-0.031301	3.217854
156.583169	3459.558134	6.413286	-0.031325	3.221383
156.836577	3467.565187	6.418291	-0.031377	3.224903
156.810839	3475.644133	6.423296	-0.031378	3.228439
157.104840	3483.681601	6.428301	-0.031438	3.231966
157.533312	3491.742745	6.433306	-0.031523	3.235504
157.714651	3499.704011	6.438310	-0.031562	3.238986
158.206437	3507.711296	6.443315	-0.031659	3.242496
158.228539	3515.744815	6.448320	-0.031668	3.245995
158.153734	3523.789438	6.453325	-0.031659	3.249491
158.346147	3531.854206	6.458330	-0.031701	3.253002
158.715133	3539.874972	6.463334	-0.031775	3.256498
158.802405	3547.885524	6.468339	-0.031796	3.259974
159.046914	3555.893997	6.473344	-0.031847	3.263452
159.232792	3563.920788	6.478349	-0.031887	3.266932
159.613983	3571.950131	6.483354	-0.031963	3.270417
159.909876	3580.011852	6.488358	-0.032023	3.273908
159.968792	3588.055143	6.493363	-0.032040	3.277379
159.931960	3596.081520	6.498368	-0.032038	3.280835
160.262896	3604.082642	6.503373	-0.032105	3.284291
160.326150	3612.147559	6.508378	-0.032122	3.287760
160.504817	3620.157625	6.513382	-0.032161	3.291206
160.693264	3628.206623	6.518387	-0.032201	3.294666
160.750577	3636.217519	6.523392	-0.032217	3.298101
161.104933	3644.196588	6.528397	-0.032288	3.301530
161.396437	3652.217453	6.533402	-0.032348	3.304971
161.500458	3660.267038	6.538406	-0.032372	3.308413
161.839073	3668.349780	6.543411	-0.032441	3.311875
161.871189	3676.392617	6.548416	-0.032452	3.315304
162.173290	3684.372442	6.553421	-0.032514	3.318714
162.250609	3692.423622	6.558426	-0.032533	3.322141
162.564199	3700.395637	6.563430	-0.032597	3.325540
162.965189	3708.434579	6.568435	-0.032677	3.328968
163.096589	3716.475976	6.573440	-0.032707	3.332383
163.213793	3724.535036	6.578445	-0.032734	3.335801
163.172140	3732.572623	6.583450	-0.032731	3.339201
163.438235	3740.585169	6.588454	-0.032786	3.342598
163.617677	3748.628257	6.593459	-0.032825	3.346001
163.746607	3756.645470	6.598464	-0.032854	3.349388
164.184769	3764.685112	6.603469	-0.032941	3.352792
164.083988	3772.774801	6.608474	-0.032927	3.356195
164.096130	3780.715975	6.613478	-0.032935	3.359535
164.258037	3788.795042	6.618483	-0.032970	3.362936
164.368097	3796.814594	6.623488	-0.032996	3.366306
164.538024	3804.795454	6.628493	-0.033033	3.369659
164.774671	3812.890553	6.633498	-0.033082	3.373058
165.009074	3820.915758	6.638502	-0.033131	3.376425
165.273504	3828.932369	6.643507	-0.033186	3.379786
165.461751	3836.922357	6.648512	-0.033226	3.383129
165.724156	3844.944826	6.653517	-0.033280	3.386486
165.938433	3852.986903	6.658522	-0.033326	3.389846
166.073800	3861.051150	6.663526	-0.033356	3.393208
166.316940	3869.136277	6.668531	-0.033407	3.396580
166.323152	3877.091387	6.673536	-0.033413	3.399886
166.444640	3885.098122	6.678541	-0.033441	3.403215
166.692587	3893.100806	6.683546	-0.033492	3.406542
166.601687	3901.114490	6.688550	-0.033481	3.409860
166.790641	3909.190652	6.693555	-0.033521	3.413209
166.692355	3917.244779	6.698560	-0.033508	3.416537
167.124476	3925.195272	6.703565	-0.033594	3.419836
167.497890	3933.219745	6.708570	-0.033669	3.423161
167.215156	3941.307152	6.713574	-0.033621	3.426486
167.692711	3949.282138	6.718579	-0.033716	3.429787
168.027403	3957.303182	6.723584	-0.033783	3.433099
168.482300	3965.307224	6.728589	-0.033873	3.436405
168.691841	3973.335941	6.733594	-0.033917	3.439710
168.737745	3981.343023	6.738598	-0.033931	3.442997
168.651612	3989.439242	6.743603	-0.033921	3.446313
168.608468	3997.498601	6.748608	-0.033918	3.449613
169.089694	4005.442864	6.753613	-0.034013	3.452879
169.536928	4013.503038	6.758618	-0.034101	3.456188
169.434105	4021.532264	6.763622	-0.034087	3.459464
169.812418	4029.579149	6.768627	-0.034163	3.462759
169.911235	4037.577056	6.773632	-0.034187	3.466022
170.279213	4045.620382	6.778637	-0.034261	3.469309
170.568471	4053.669266	6.783642	-0.034320	3.472593
170.443498	4061.743053	6.788646	-0.034302	3.475870
170.874929	4069.696232	6.793651	-0.034387	3.479114
170.920145	4077.720309	6.798656	-0.034401	3.482370
171.246036	4085.714647	6.803661	-0.034467	3.485620
171.729011	4093.735257	6.808666	-0.034562	3.488883
171.889274	4101.767771	6.813670	-0.034597	3.492138
171.785799	4109.856073	6.818675	-0.034583	3.495403
171.920199	4117.878630	6.823680	-0.034614	3.498647
172.115135	4125.866105	6.828685	-0.034655	3.501875
172.342216	4133.853931	6.833690	-0.034703	3.505101
172.819781	4141.844799	6.838694	-0.034797	3.508333
172.957598	4149.935197	6.843699	-0.034828	3.511592
173.044594	4157.946120	6.848704	-0.034849	3.514814
173.430648	4165.978293	6.853709	-0.034926	3.518051
173.644399	4174.009299	6.858714	-0.034972	3.521279
173.595905	4181.988100	6.863718	-0.034968	3.524476
173.639815	4190.085732	6.868723	-0.034981	3.527719
173.987096	4198.091531	6.873728	-0.035051	3.530933
174.448865	4206.111840	6.878733	-0.035142	3.534152
174.646288	4214.167265	6.883738	-0.035185	3.537375
174.490638	4222.211050	6.888742	-0.035161	3.540579
174.930333	4230.198196	6.893747	-0.035248	3.543776
174.806369	4238.257313	6.898752	-0.035230	3.546981
175.036273	4246.269234	6.903757	-0.035278	3.550176
175.778284	4254.353639	6.908762	-0.035422	3.553411
175.629988	4262.414529	6.913766	-0.035399	3.556608
175.660226	4270.387644	6.918771	-0.035410	3.559772
175.880648	4278.376803	6.923776	-0.035457	3.562946
175.816069	4286.407402	6.928781	-0.035450	3.566125
175.969207	4294.439556	6.933786	-0.035484	3.569308
176.164499	4302.449037	6.938790	-0.035525	3.572480
176.492155	4310.470383	6.943795	-0.035592	3.575658
176.670637	4318.443313	6.948800	-0.035630	3.578809
176.956616	4326.456017	6.953805	-0.035689	3.581977
177.229048	4334.465825	6.958810	-0.035745	3.585140
177.487091	4342.495772	6.963814	-0.035798	3.588308
177.672138	4350.595340	6.968819	-0.035838	3.591499
177.889486	4358.556809	6.973824	-0.035883	3.594633
178.016356	4366.597798	6.978829	-0.035912	3.597793
177.973542	4374.667496	6.983834	-0.035910	3.600957
178.128381	4382.602790	6.988838	-0.035944	3.604070
178.485291	4390.660822	6.993843	-0.036015	3.607235
178.514895	4398.680425	6.998848	-0.036026	3.610373
178.647599	4406.730970	7.003853	-0.036056	3.613523
179.038199	4414.777793	7.008858	-0.036134	3.616676
179.118233	4422.715760	7.013862	-0.036154	3.619775
179.410164	4430.775655	7.018867	-0.036214	3.622925
179.421221	4438.828476	7.023872	-0.036221	3.626062
179.609271	4446.822283	7.028877	-0.036262	3.629178
179.631167	4454.967043	7.033882	-0.036271	3.632345
179.774941	4462.942517	7.038886	-0.036303	3.635447
179.856001	4470.972624	7.043891	-0.036324	3.638566
180.064030	4478.969585	7.048896	-0.036368	3.641673
179.916087	4486.944509	7.053901	-0.036345	3.644759
180.570060	4494.968506	7.058906	-0.036472	3.647882
180.409487	4503.037863	7.063910	-0.036448	3.650999
181.222839	4511.005483	7.068915	-0.036604	3.654100
181.005414	4519.101381	7.073920	-0.036569	3.657220
181.337785	4527.048205	7.078925	-0.036636	3.660295
181.596166	4535.108908	7.083930	-0.036690	3.663409
181.811721	4543.088624	7.088934	-0.036735	3.666487
181.992100	4551.163523	7.093939	-0.036774	3.669599
182.139055	4559.214278	7.098944	-0.036807	3.672699
182.277343	4567.237519	7.103949	-0.036838	3.675784
182.544940	4575.254979	7.108954	-0.036893	3.678869
182.589317	4583.249175	7.113958	-0.036906	3.681936
182.840431	4591.245481	7.118963	-0.036958	3.685006
182.952057	4599.292767	7.123968	-0.036984	3.688090
183.062872	4607.324854	7.128973	-0.037010	3.691166
183.502050	4615.366070	7.133978	-0.037097	3.694250
183.562824	4623.346297	7.138982	-0.037114	3.697299
184.012963	4631.366126	7.143987	-0.037203	3.700371
184.174236	4639.368000	7.148992	-0.037238	3.703426
184.309818	4647.415921	7.153997	-0.037269	3.706495
184.837580	4655.455344	7.159002	-0.037372	3.709568
184.751668	4663.555588	7.164006	-0.037362	3.712647
185.038911	4671.600175	7.169011	-0.037421	3.715711
184.923861	4679.597239	7.174016	-0.037404	3.718744
185.377343	4687.578869	7.179021	-0.037494	3.721783
185.853416	4695.483414	7.184026	-0.037588	3.724791
185.789515	4703.548859	7.189030	-0.037581	3.727844
186.214860	4711.549012	7.194035	-0.037666	3.730882
186.613599	4719.572408	7.199040	-0.037745	3.733925
186.603299	4727.671786	7.204045	-0.037749	3.736985
187.076286	4735.656838	7.209050	-0.037842	3.740011
187.662152	4743.652362	7.214054	-0.037956	3.743040
187.732316	4751.685568	7.219059	-0.037975	3.746069
188.006592	4759.740980	7.224064	-0.038031	3.749109
188.550914	4767.775743	7.229069	-0.038138	3.752145
188.856099	4775.817727	7.234074	-0.038200	3.755176
189.140308	4783.804439	7.239078	-0.038258	3.758183
189.432891	4791.865403	7.244083	-0.038318	3.761215
189.597717	4799.821644	7.249088	-0.038354	3.764203
189.734893	4807.836788	7.254093	-0.038385	3.767210
189.853255	4815.917086	7.259098	-0.038412	3.770238
190.342781	4823.892415	7.264102	-0.038508	3.773233
190.695225	4831.957667	7.269107	-0.038579	3.776256
190.975560	4839.958581	7.274112	-0.038637	3.779251
191.024856	4847.977146	7.279117	-0.038651	3.782245
191.231807	4856.001161	7.284122	-0.038695	3.785242
191.348599	4863.998386	7.289126	-0.038722	3.788225
191.781463	4872.047183	7.294131	-0.038808	3.791231
191.872592	4880.146046	7.299136	-0.038830	3.794246
192.089910	4888.134833	7.304141	-0.038876	3.797221
192.512358	4896.143301	7.309146	-0.038960	3.800205
192.574615	4904.122719	7.314150	-0.038977	3.803168
192.667108	4912.164756	7.319155	-0.038999	3.806153
192.625069	4920.219199	7.324160	-0.038997	3.809137
192.962297	4928.222802	7.329165	-0.039065	3.812108
193.223690	4936.220250	7.334170	-0.039119	3.815072
193.365188	4944.235928	7.339174	-0.039150	3.818039
193.608501	4952.263974	7.344179	-0.039201	3.821010
193.721295	4960.276987	7.349184	-0.039227	3.823970
193.813571	4968.294880	7.354189	-0.039250	3.826929
193.634349	4976.389337	7.359194	-0.039222	3.829909
194.166270	4984.344270	7.364198	-0.039326	3.832850
194.581359	4992.351948	7.369203	-0.039408	3.835805
194.550401	5000.383951	7.374208	-0.039408	3.838758
194.921258	5008.401610	7.379213	-0.039482	3.841711
194.920002	5016.446965	7.384218	-0.039487	3.844665
195.276499	5024.458437	7.389222	-0.039559	3.847611
195.712478	5032.474418	7.394227	-0.039645	3.850558
195.942123	5040.489229	7.399232	-0.039693	3.853499
196.152311	5048.524124	7.404237	-0.039738	3.856444
196.285366	5056.556626	7.409242	-0.039768	3.859384
196.557001	5064.535712	7.414246	-0.039824	3.862305
196.608491	5072.582400	7.419251	-0.039839	3.865244
196.582776	5080.624824	7.424256	-0.039839	3.868179
196.931148	5088.648258	7.429261	-0.039909	3.871111
197.126883	5096.908933	7.434266	-0.039951	3.874124
197.542421	5104.833337	7.439270	-0.040034	3.877017
197.440692	5112.789414	7.444275	-0.040020	3.879909
197.692480	5120.798970	7.449280	-0.040072	3.882825
198.082475	5128.711984	7.454285	-0.040150	3.885707
198.392653	5136.730726	7.459290	-0.040213	3.888623
198.555144	5144.736607	7.464294	-0.040249	3.891530
198.814284	5152.812492	7.469299	-0.040302	3.894461
198.805637	5160.877343	7.474304	-0.040306	3.897382
198.716085	5168.868682	7.479309	-0.040294	3.900272
198.873516	5176.920649	7.484314	-0.040329	3.903186
199.275813	5184.847804	7.489318	-0.040409	3.906058
199.852283	5192.848249	7.494323	-0.040522	3.908957
199.807799	5200.979798	7.499328	-0.040519	3.911890
199.878042	5208.990369	7.504333	-0.040537	3.914779
200.084761	5217.006113	7.509338	-0.040581	3.917670
200.210456	5224.989412	7.514342	-0.040610	3.920546
200.636051	5232.967171	7.519347	-0.040694	3.923423
200.588792	5241.056980	7.524352	-0.040691	3.926330
201.205661	5248.989522	7.529357	-0.040811	3.929190
201.922574	5257.021526	7.534362	-0.040949	3.932086
201.839000	5265.078972	7.539366	-0.040939	3.934974
202.366309	5273.079370	7.544371	-0.041043	3.937850
202.753111	5281.070007	7.549376	-0.041120	3.940718
202.745119	5289.104958	7.554381	-0.041124	3.943593
203.080532	5297.140569	7.559386	-0.041191	3.946472
203.295530	5305.137286	7.564390	-0.041237	3.949333
203.703056	5313.187549	7.569395	-0.041318	3.952215
203.851788	5321.239565	7.574400	-0.041351	3.955090
203.840952	5329.237629	7.579405	-0.041354	3.957941
204.081512	5337.281308	7.584410	-0.041404	3.960811
204.183468	5345.258498	7.589414	-0.041428	3.963653
204.407295	5353.281404	7.594419	-0.041475	3.966511
204.690306	5361.281081	7.599424	-0.041533	3.969359
204.509686	5369.385540	7.604429	-0.041505	3.972235
204.804673	5377.391978	7.609434	-0.041565	3.975082
204.775409	5385.419226	7.614438	-0.041565	3.977929
204.771101	5393.445788	7.619443	-0.041570	3.980774
205.120507	5401.416975	7.624448	-0.041640	3.983603
204.920734	5409.510724	7.629453	-0.041608	3.986465
205.144054	5417.566330	7.634458	-0.041655	3.989318
205.898831	5425.431539	7.639462	-0.041801	3.992110
205.625170	5433.568922	7.644467	-0.041755	3.994980
206.296510	5441.477794	7.649472	-0.041885	3.997782
206.773762	5449.423279	7.654477	-0.041979	4.000591
207.281202	5457.486650	7.659482	-0.042079	4.003441
207.523319	5465.489653	7.664486	-0.042129	4.006263
207.961672	5473.519966	7.669491	-0.042216	4.009096
207.944756	5481.585820	7.674496	-0.042218	4.011933
208.073472	5489.667931	7.679501	-0.042248	4.014775
208.629046	5497.699103	7.684506	-0.042357	4.017604
208.634270	5505.655782	7.689510	-0.042363	4.020396
209.065604	5513.685210	7.694515	-0.042448	4.023218
209.313583	5521.705127	7.699520	-0.042500	4.026033
209.409598	5529.751500	7.704525	-0.042523	4.028852
209.743856	5537.791688	7.709530	-0.042590	4.031670
209.701705	5545.926743	7.714534	-0.042588	4.034514
210.100014	5553.923044	7.719539	-0.042667	4.037315
210.285608	5561.840042	7.724544	-0.042707	4.040082
210.553587	5569.849523	7.729549	-0.042762	4.042881
210.696124	5577.852844	7.734554	-0.042794	4.045674
210.621091	5585.868924	7.739558	-0.042785	4.048466
210.745995	5593.894881	7.744563	-0.042814	4.051263
210.942744	5601.955825	7.749568	-0.042856	4.054071
211.260599	5609.996881	7.754573	-0.042920	4.056871
211.604478	5617.923055	7.759578	-0.042990	4.059631
211.746843	5625.975284	7.764582	-0.043021	4.062429
212.046311	5633.970155	7.769587	-0.043082	4.065207
211.889570	5642.037405	7.774592	-0.043059	4.068003
212.178388	5649.998788	7.779597	-0.043118	4.070766
212.224472	5658.111441	7.784602	-0.043132	4.073576
212.502518	5666.111439	7.789606	-0.043189	4.076348
212.574968	5674.101543	7.794611	-0.043207	4.079113
212.714424	5682.154148	7.799616	-0.043239	4.081897
212.893593	5690.050725	7.804621	-0.043277	4.084627
213.455880	5698.106267	7.809626	-0.043387	4.087415
213.383680	5706.113915	7.814630	-0.043379	4.090175
213.418392	5714.197191	7.819635	-0.043391	4.092962
213.640259	5722.229956	7.824640	-0.043437	4.095731
213.945720	5730.144432	7.829645	-0.043499	4.098459
214.209994	5738.239284	7.834650	-0.043554	4.101247
214.406657	5746.205078	7.839654	-0.043596	4.103987
214.345913	5754.270373	7.844659	-0.043590	4.106757
214.733758	5762.247238	7.849664	-0.043667	4.109500
214.769919	5770.313500	7.854669	-0.043679	4.112267
215.351050	5778.381763	7.859674	-0.043793	4.115040
215.699084	5786.311000	7.864678	-0.043863	4.117761
215.898313	5794.322155	7.869683	-0.043905	4.120506
216.128119	5802.376903	7.874688	-0.043953	4.123264
216.430845	5810.354156	7.879693	-0.044015	4.125995
216.509870	5818.396865	7.884698	-0.044035	4.128743
216.858543	5826.442787	7.889702	-0.044105	4.131494
217.075578	5834.478700	7.894707	-0.044151	4.134239
217.253714	5842.513163	7.899712	-0.044189	4.136980
217.593323	5850.491527	7.904717	-0.044258	4.139703
217.390859	5858.560931	7.909722	-0.044225	4.142448
217.612796	5866.513682	7.914726	-0.044272	4.145156
217.857480	5874.569231	7.919731	-0.044323	4.147898
218.118258	5882.600265	7.924736	-0.044377	4.150630
218.214287	5890.620184	7.929741	-0.044400	4.153355
218.524672	5898.662166	7.934746	-0.044463	4.156088
218.787068	5906.634742	7.939750	-0.044517	4.158795
218.731342	5914.681208	7.944755	-0.044512	4.161521
218.862085	5922.655801	7.949760	-0.044541	4.164223
219.133405	5930.676251	7.954765	-0.044597	4.166941
219.445182	5938.717361	7.959770	-0.044661	4.169664
219.392400	5946.760860	7.964774	-0.044656	4.172383
219.787056	5954.730508	7.969779	-0.044735	4.175079
219.994991	5962.806724	7.974784	-0.044779	4.177808
220.052945	5970.761618	7.979789	-0.044795	4.180492
220.268281	5978.781538	7.984794	-0.044840	4.183198
220.487430	5986.789944	7.989798	-0.044886	4.185899
220.557441	5994.840724	7.994803	-0.044905	4.188610
220.728454	6002.844444	7.999808	-0.044942	4.191305
220.948553	6010.985622	8.004813	-0.044988	4.194045
221.348615	6018.990114	8.009818	-0.045068	4.196739
221.370689	6026.934204	8.014822	-0.045077	4.199407
221.788649	6034.944942	8.019827	-0.045160	4.202100
221.945266	6042.907368	8.024832	-0.045195	4.204772
222.054095	6050.908032	8.029837	-0.045220	4.207455
222.425440	6058.943390	8.034842	-0.045295	4.210150
222.676471	6066.974529	8.039846	-0.045347	4.212841
222.936769	6074.992905	8.044851	-0.045400	4.215526
222.997744	6083.042834	8.049856	-0.045417	4.218217
223.139954	6091.019885	8.054861	-0.045449	4.220884
223.768943	6099.015263	8.059866	-0.045571	4.223560
223.839915	6107.053338	8.064870	-0.045590	4.226242
224.056801	6115.026886	8.069875	-0.045635	4.228903
224.034341	6123.150011	8.074880	-0.045636	4.231610
224.171587	6131.137925	8.079885	-0.045667	4.234271
224.387832	6139.242289	8.084890	-0.045713	4.236971
224.499200	6147.146345	8.089894	-0.045739	4.239601
224.741667	6155.161720	8.094899	-0.045789	4.242267
225.032742	6163.181874	8.099904	-0.045849	4.244934
225.303398	6171.174820	8.104909	-0.045904	4.247590
225.596031	6179.236312	8.109914	-0.045964	4.250267
225.837818	6187.236540	8.114918	-0.046014	4.252922
226.044480	6195.272010	8.119923	-0.046058	4.255586
226.350730	6203.290214	8.124928	-0.046120	4.258244
226.379549	6211.320721	8.129933	-0.046131	4.260902
226.799427	6219.307527	8.134938	-0.046215	4.263546
227.150185	6227.326742	8.139942	-0.046285	4.266200
227.494240	6235.352214	8.144947	-0.046354	4.268854
227.492054	6243.431230	8.149952	-0.046359	4.271520
227.387656	6251.498907	8.154957	-0.046345	4.274181
228.060534	6259.454859	8.159962	-0.046476	4.276809
228.098368	6267.409705	8.164966	-0.046488	4.279431
228.385214	6275.455414	8.169971	-0.046547	4.282082
228.653576	6283.452583	8.174976	-0.046602	4.284716
228.761363	6291.473814	8.179981	-0.046627	4.287355
229.070524	6299.491474	8.184986	-0.046690	4.289992
229.056715	6307.537941	8.189990	-0.046693	4.292635
229.296421	6315.578715	8.194995	-0.046743	4.295276
229.684386	6323.581141	8.200000	-0.046820	4.297904
229.736855	6331.591540	8.205005	-0.046835	4.300531
229.995245	6339.630791	8.210010	-0.046889	4.303167
229.989852	6347.593267	8.215014	-0.046893	4.305774
230.088452	6355.679458	8.220019	-0.046917	4.308421
230.224484	6363.684855	8.225024	-0.046947	4.311040
230.395615	6371.684860	8.230029	-0.046984	4.313656
230.388272	6379.725220	8.235034	-0.046988	4.316282
230.588633	6387.697136	8.240038	-0.047031	4.318886
230.591284	6395.756658	8.245043	-0.047037	4.321515
230.992578	6403.715944	8.250048	-0.047117	4.324113
231.305411	6411.709829	8.255053	-0.047180	4.326720
231.411043	6419.770501	8.260058	-0.047205	4.329345
231.275841	6427.881360	8.265062	-0.047185	4.331984
231.722516	6435.764456	8.270067	-0.047274	4.334551
231.947546	6443.836532	8.275072	-0.047321	4.337176
232.213507	6451.771465	8.280077	-0.047376	4.339755
232.300299	6459.900419	8.285082	-0.047397	4.342395
232.337824	6467.861110	8.290086	-0.047409	4.344978
232.851567	6475.871288	8.295091	-0.047510	4.347579
233.011074	6483.891328	8.300096	-0.047545	4.350179
233.116934	6491.969324	8.305101	-0.047570	4.352796
233.641693	6500.035700	8.310106	-0.047673	4.355410
233.893429	6508.000214	8.315110	-0.047725	4.357988
233.736454	6515.947105	8.320115	-0.047701	4.360556
234.118194	6524.006770	8.325120	-0.047778	4.363162
234.204747	6531.934542	8.330125	-0.047799	4.365722
234.462513	6539.980099	8.335130	-0.047852	4.368320
234.651879	6548.039504	8.340134	-0.047893	4.370921
234.873788	6556.082882	8.345139	-0.047940	4.373514
235.061063	6564.103611	8.350144	-0.047980	4.376099
235.096249	6572.081303	8.355149	-0.047991	4.378668
235.252028	6580.111181	8.360154	-0.048026	4.381252
235.551566	6588.108523	8.365158	-0.048087	4.383825
235.567882	6596.095897	8.370163	-0.048095	4.386392
235.881821	6604.140515	8.375168	-0.048159	4.388977
236.017939	6612.158801	8.380173	-0.048189	4.391552
236.344252	6620.268415	8.385178	-0.048256	4.394155
236.524367	6628.231350	8.390182	-0.048294	4.396709
236.761988	6636.171793	8.395187	-0.048344	4.399254
237.087818	6644.269685	8.400192	-0.048410	4.401849
237.248955	6652.190535	8.405197	-0.048445	4.404384
237.530067	6660.257773	8.410202	-0.048503	4.406966
237.659892	6668.240238	8.415206	-0.048532	4.409518
237.671186	6676.292637	8.420211	-0.048539	4.412091
238.011527	6684.376369	8.425216	-0.048608	4.414673
237.920192	6692.386864	8.430221	-0.048596	4.417229
238.393225	6700.381437	8.435226	-0.048690	4.419781
238.398132	6708.395046	8.440230	-0.048696	4.422335
238.634648	6716.359205	8.445235	-0.048745	4.424873
239.033989	6724.420057	8.450240	-0.048825	4.427440
239.069806	6732.442400	8.455245	-0.048837	4.429993
239.294578	6740.475806	8.460250	-0.048884	4.432548
239.458489	6748.555005	8.465254	-0.048920	4.435116
239.727942	6756.495073	8.470259	-0.048975	4.437639
239.961755	6764.513015	8.475264	-0.049024	4.440185
240.122373	6772.514886	8.480269	-0.049059	4.442724
240.289596	6780.493748	8.485274	-0.049096	4.445255
240.355607	6788.549371	8.490278	-0.049113	4.447808
240.527823	6796.561104	8.495283	-0.049151	4.450346
240.719414	6804.628577	8.500288	-0.049192	4.452900
240.642383	6812.616863	8.505293	-0.049182	4.455426
241.012135	6820.643325	8.510298	-0.049257	4.457965
241.197809	6828.649799	8.515302	-0.049296	4.460496
241.496151	6836.659719	8.520307	-0.049357	4.463026
241.649043	6844.623364	8.525312	-0.049391	4.465540
241.974985	6852.681895	8.530317	-0.049457	4.468083
242.189340	6860.712578	8.535322	-0.049502	4.470615
242.421079	6868.761616	8.540326	-0.049551	4.473151
242.429532	6876.735126	8.545331	-0.049557	4.475662
242.731077	6884.802685	8.550336	-0.049619	4.478202
242.679266	6892.741150	8.555341	-0.049614	4.480699
243.039718	6900.797584	8.560346	-0.049687	4.483232
243.036588	6908.764480	8.565351	-0.049691	4.485735
243.257563	6916.797576	8.570355	-0.049738	4.488258
243.349935	6924.844320	8.575360	-0.049760	4.490783
243.600521	6932.845562	8.580365	-0.049812	4.493293
243.795508	6940.885700	8.585370	-0.049854	4.495814
243.840447	6948.891722	8.590375	-0.049868	4.498322
244.001770	6956.879419	8.595379	-0.049903	4.500824
244.250344	6964.923882	8.600384	-0.049954	4.503342
244.369949	6972.906974	8.605389	-0.049982	4.505839
244.784647	6980.936459	8.610394	-0.050064	4.508349
245.174853	6988.927774	8.615399	-0.050142	4.510847
245.358501	6997.019053	8.620403	-0.050182	4.513373
245.304377	7005.049406	8.625408	-0.050177	4.515879
245.412465	7013.007105	8.630413	-0.050202	4.518361
245.733824	7021.005028	8.635418	-0.050268	4.520854
245.863381	7028.996578	8.640423	-0.050297	4.523344
246.134728	7037.001831	8.645427	-0.050353	4.525837
246.416213	7045.044676	8.650432	-0.050410	4.528340
246.232545	7053.043288	8.655437	-0.050381	4.530828
246.504167	7061.097211	8.660442	-0.050437	4.533332
246.701020	7069.135955	8.665447	-0.050479	4.535829
246.903082	7077.115827	8.670451	-0.050522	4.538307
246.958621	7085.147083	8.675456	-0.050538	4.540799
247.153747	7093.132857	8.680461	-0.050579	4.543276
247.255547	7101.187925	8.685466	-0.050604	4.545773
247.407603	7109.173693	8.690471	-0.050637	4.548248
247.723112	7117.181443	8.695475	-0.050701	4.550727
248.047575	7125.317787	8.700480	-0.050767	4.553246
247.987587	7133.272202	8.705485	-0.050761	4.555706
248.211839	7141.289648	8.710490	-0.050808	4.558184
248.438777	7149.273137	8.715495	-0.050856	4.560651
248.705142	7157.249816	8.720499	-0.050910	4.563114
248.955769	7165.254230	8.725504	-0.050962	4.565585
249.060941	7173.281635	8.730509	-0.050987	4.568061
249.185362	7181.318470	8.735514	-0.051016	4.570538
249.419231	7189.394998	8.740519	-0.051065	4.573027
249.436094	7197.413504	8.745523	-0.051073	4.575496
249.777850	7205.452124	8.750528	-0.051142	4.577970
249.494691	7213.380278	8.755533	-0.051094	4.580409
249.690817	7221.431910	8.760538	-0.051136	4.582884
249.892085	7229.384311	8.765543	-0.051179	4.585328
250.160535	7237.453869	8.770547	-0.051234	4.587806
250.475036	7245.480065	8.775552	-0.051298	4.590270
250.612717	7253.538236	8.780557	-0.051329	4.592742
250.964499	7261.579408	8.785562	-0.051400	4.595207
251.206667	7269.567962	8.790567	-0.051450	4.597655
251.202377	7277.477184	8.795571	-0.051454	4.600077
251.521253	7285.563161	8.800576	-0.051519	4.602553
251.683071	7293.476924	8.805581	-0.051555	4.604974
251.741767	7301.616445	8.810586	-0.051571	4.607463
251.795656	7309.587704	8.815591	-0.051586	4.609899
251.926961	7317.656345	8.820595	-0.051616	4.612363
252.247193	7325.646789	8.825600	-0.051681	4.614802
252.225791	7333.692186	8.830605	-0.051682	4.617257
252.474126	7341.632807	8.835610	-0.051734	4.619679
252.671224	7349.713858	8.840615	-0.051776	4.622142
252.684734	7357.664594	8.845619	-0.051783	4.624564
253.119827	7365.712868	8.850624	-0.051870	4.627014
253.228013	7373.687745	8.855629	-0.051895	4.629441
253.308351	7381.729407	8.860634	-0.051915	4.631886
253.469911	7389.799237	8.865639	-0.051951	4.634339
253.725329	7397.812050	8.870643	-0.052003	4.636773
254.028623	7405.784099	8.875648	-0.052065	4.639194
254.136564	7413.798821	8.880653	-0.052091	4.641626
254.454790	7421.771253	8.885658	-0.052155	4.644044
254.587956	7429.847134	8.890663	-0.052185	4.646493
254.451202	7437.802516	8.895667	-0.052165	4.648903
254.658218	7445.871779	8.900672	-0.052209	4.651347
254.958519	7453.875656	8.905677	-0.052270	4.653769
254.988024	7461.912450	8.910682	-0.052281	4.656201
255.095186	7469.917710	8.915687	-0.052306	4.658621
254.995159	7477.918865	8.920691	-0.052293	4.661040
255.221624	7485.940391	8.925696	-0.052340	4.663462
255.203474	7493.917228	8.930701	-0.052342	4.665871
255.600396	7501.973048	8.935706	-0.052421	4.668301
255.691233	7510.024136	8.940711	-0.052443	4.670729
255.985847	7518.073474	8.945715	-0.052503	4.673154
256.037532	7526.143179	8.950720	-0.052518	4.675586
256.086646	7534.123759	8.955725	-0.052533	4.677989
256.186290	7542.046557	8.960730	-0.052557	4.680373
256.394015	7550.085279	8.965735	-0.052601	4.682791
256.840348	7558.020902	8.970739	-0.052689	4.685175
257.054924	7566.048406	8.975744	-0.052734	4.687587
256.917203	7574.048348	8.980749	-0.052714	4.689990
257.215581	7582.115042	8.985754	-0.052775	4.692411
257.678636	7590.093665	8.990759	-0.052866	4.694804
257.590348	7598.116813	8.995763	-0.052855	4.697210
257.782604	7606.158903	9.000768	-0.052896	4.699620
257.985452	7614.199040	9.005773	-0.052939	4.702028
257.968131	7622.148627	9.010778	-0.052941	4.704408
258.352591	7630.239417	9.015783	-0.053018	4.706828
258.656892	7638.178228	9.020787	-0.053080	4.709202
258.948547	7646.242225	9.025792	-0.053139	4.711612
258.792119	7654.242434	9.030797	-0.053116	4.714002
259.296404	7662.320023	9.035802	-0.053215	4.716413
259.635268	7670.256970	9.040807	-0.053283	4.718781
259.602342	7678.293709	9.045811	-0.053282	4.721179
259.860951	7686.322885	9.050816	-0.053336	4.723572
259.976586	7694.340063	9.055821	-0.053362	4.725961
260.154475	7702.385084	9.060826	-0.053401	4.728357
260.132313	7710.400606	9.065831	-0.053402	4.730744
260.261384	7718.366240	9.070835	-0.053431	4.733113
260.402776	7726.434760	9.075840	-0.053463	4.735513
260.535630	7734.434852	9.080845	-0.053493	4.737890
260.901739	7742.394461	9.085850	-0.053566	4.740254
261.171924	7750.454844	9.090855	-0.053622	4.742647
260.936100	7758.407016	9.095859	-0.053583	4.745008
261.328759	7766.512909	9.100864	-0.053662	4.747411
261.584343	7774.456009	9.105869	-0.053715	4.749766
261.838769	7782.512725	9.110874	-0.053767	4.752152
262.010750	7790.584132	9.115879	-0.053805	4.754543
262.363409	7798.576606	9.120883	-0.053875	4.756908
262.792272	7806.563662	9.125888	-0.053961	4.759269
262.809168	7814.565136	9.130893	-0.053969	4.761636
262.916018	7822.577119	9.135898	-0.053994	4.764004
262.903302	7830.595704	9.140903	-0.053997	4.766373
263.049444	7838.571879	9.145907	-0.054030	4.768728
263.156516	7846.640370	9.150912	-0.054055	4.771109
263.263115	7854.664244	9.155917	-0.054080	4.773476
263.449540	7862.673200	9.160922	-0.054120	4.775837
263.752446	7870.688991	9.165927	-0.054182	4.778198
264.094410	7878.653276	9.170931	-0.054250	4.780543
264.275529	7886.748549	9.175936	-0.054290	4.782925
264.383046	7894.682323	9.180941	-0.054315	4.785260
264.414876	7902.705891	9.185946	-0.054326	4.787620
264.695110	7910.746936	9.190951	-0.054383	4.789982
264.857035	7918.772102	9.195955	-0.054419	4.792340
264.948600	7926.779945	9.200960	-0.054441	4.794691
265.132294	7934.858168	9.205965	-0.054481	4.797062
265.387608	7942.743698	9.210970	-0.054533	4.799374
265.610289	7950.873236	9.215975	-0.054580	4.801757
265.605635	7958.759069	9.220979	-0.054585	4.804069
265.888940	7966.858314	9.225984	-0.054643	4.806440
265.874054	7974.808250	9.230989	-0.054645	4.808768
266.016831	7982.900318	9.235994	-0.054677	4.811136
266.349926	7990.389252	9.240999	-0.054744	4.813325
266.304349	7994.959778	9.246003	-0.054739	4.814662

266.493210	7997.474645	9.251008	-0.054775	4.815396
266.491117	7998.700591	9.256013	-0.054776	4.815755
266.692981	7999.379204	9.261018	-0.054814	4.815952
266.703473	7999.726507	9.266023	-0.054816	4.816054
266.732107	7999.725960	9.271027	-0.054822	4.816053
266.865385	7999.737981	9.276032	-0.054846	4.816056
266.960652	7999.711936	9.281037	-0.054864	4.816048
267.157472	7999.743261	9.286042	-0.054901	4.816056
267.097513	7999.769953	9.291047	-0.054890	4.816064
267.309033	7999.755617	9.296051	-0.054929	4.816059
267.332854	7999.760324	9.301056	-0.054934	4.816060
267.215883	7999.870364	9.306061	-0.054912	4.816093
267.571830	7999.969715	9.311066	-0.054978	4.816120
267.533067	7999.876098	9.316071	-0.054971	4.816093
267.533274	7999.995731	9.321075	-0.054971	4.816128
267.531279	7999.771405	9.326080	-0.054971	4.816062
267.728617	8000.036650	9.331085	-0.055008	4.816139
267.673072	7999.872236	9.336090	-0.054997	4.816091
267.712173	7999.860129	9.341095	-0.055005	4.816087
267.702867	7999.980659	9.346099	-0.055003	4.816123
267.807857	7999.871479	9.351104	-0.055023	4.816090
267.710686	7999.766127	9.356109	-0.055005	4.816060
267.756621	7999.957078	9.361114	-0.055013	4.816115
267.727547	7999.872180	9.366119	-0.055008	4.816091
267.777738	8000.007668	9.371123	-0.055017	4.816130
267.909144	7999.783613	9.376128	-0.055042	4.816064
268.026001	7999.869037	9.381133	-0.055064	4.816088
268.126065	7999.782197	9.386138	-0.055082	4.816062
268.136276	7999.903079	9.391143	-0.055084	4.816098
268.098179	7999.895988	9.396147	-0.055077	4.816096
268.179176	7999.875025	9.401152	-0.055092	4.816089
267.985228	7999.852303	9.406157	-0.055056	4.816084
268.053883	7999.899475	9.411162	-0.055069	4.816097
268.173086	7999.868521	9.416167	-0.055091	4.816087
268.021838	7999.891429	9.421171	-0.055063	4.816095
268.243485	7999.887959	9.426176	-0.055105	4.816093
268.433071	7999.890318	9.431181	-0.055140	4.816092
268.311100	7999.887053	9.436186	-0.055117	4.816092
268.345722	7999.882342	9.441191	-0.055124	4.816090
268.274617	7999.882132	9.446195	-0.055111	4.816091
268.457827	7999.887580	9.451200	-0.055145	4.816091
268.132783	7999.879581	9.456205	-0.055084	4.816091
268.073407	8000.023773	9.461210	-0.055073	4.816133
268.249910	7999.879569	9.466215	-0.055106	4.816090
268.194004	8000.050527	9.471219	-0.055096	4.816140
268.314923	7999.791033	9.476224	-0.055118	4.816064
268.561829	7999.973867	9.481229	-0.055164	4.816116
268.584126	7999.792698	9.486234	-0.055169	4.816063
268.674053	7999.907544	9.491239	-0.055185	4.816096
268.526454	7999.898475	9.496243	-0.055158	4.816094
268.806575	7999.797796	9.501248	-0.055210	4.816063
268.558179	7999.881968	9.506253	-0.055164	4.816089
268.662698	7999.944742	9.511258	-0.055183	4.816107
268.804400	7999.922739	9.516263	-0.055210	4.816100
268.583387	7999.982839	9.521267	-0.055169	4.816118
268.690262	7999.888645	9.526272	-0.055189	4.816090
268.740759	7999.899174	9.531277	-0.055198	4.816093
268.608530	7999.817752	9.536282	-0.055174	4.816070
268.751782	7999.876953	9.541287	-0.055200	4.816087
268.711534	7999.885844	9.546291	-0.055193	4.816089
268.759863	7999.901674	9.551296	-0.055202	4.816094
268.737178	8000.004876	9.556301	-0.055198	4.816124
268.688041	7999.903591	9.561306	-0.055189	4.816095
268.813468	7999.875954	9.566311	-0.055212	4.816086
268.315941	7999.888338	9.571315	-0.055119	4.816092
268.455986	7999.846011	9.576320	-0.055146	4.816079
268.622627	7999.884272	9.581325	-0.055177	4.816089
268.437931	7999.920461	9.586330	-0.055142	4.816101
268.494430	7999.877694	9.591335	-0.055153	4.816088
268.688376	7999.929265	9.596339	-0.055189	4.816102
268.732555	7999.843552	9.601344	-0.055197	4.816077
268.522616	7999.861128	9.606349	-0.055158	4.816083
268.545198	7999.897856	9.611354	-0.055163	4.816094
269.006676	7999.883763	9.616359	-0.055249	4.816087
269.049553	7999.922994	9.621363	-0.055257	4.816099
269.042908	7999.897245	9.626368	-0.055255	4.816091
269.059154	7999.880453	9.631373	-0.055258	4.816086
268.821473	7999.994725	9.636378	-0.055214	4.816121
269.010467	7999.814429	9.641383	-0.055249	4.816067
269.073381	7999.892474	9.646387	-0.055261	4.816089
269.134708	7999.885041	9.651392	-0.055273	4.816087
269.108992	7999.911284	9.656397	-0.055268	4.816095
268.943860	7999.874127	9.661402	-0.055237	4.816085
269.168097	7999.916634	9.666407	-0.055279	4.816096
269.113451	7999.884676	9.671411	-0.055269	4.816087
269.309074	7999.898895	9.676416	-0.055305	4.816090
269.224590	8000.008458	9.681421	-0.055290	4.816123
269.079705	7999.905443	9.686426	-0.055263	4.816093
269.146091	7999.889557	9.691431	-0.055275	4.816088
269.235408	7999.999055	9.696435	-0.055292	4.816120
269.422842	7999.867862	9.701440	-0.055327	4.816080
269.299375	8000.000220	9.706445	-0.055304	4.816120
269.312552	7999.819951	9.711450	-0.055306	4.816067
269.380660	7999.910908	9.716455	-0.055319	4.816093
269.121280	7999.877389	9.721459	-0.055271	4.816085
269.210552	7999.812783	9.726464	-0.055288	4.816065
269.486591	7999.897882	9.731469	-0.055339	4.816089
269.398739	7999.989226	9.736474	-0.055323	4.816116
269.522194	7999.896398	9.741479	-0.055346	4.816088
269.356576	7999.998087	9.746483	-0.055315	4.816119
269.397899	7999.807645	9.751488	-0.055323	4.816063
269.297766	7999.972468	9.756493	-0.055304	4.816112
269.197751	7999.938622	9.761498	-0.055286	4.816102
269.548364	7999.870192	9.766503	-0.055351	4.816080
269.339540	7999.890991	9.771507	-0.055312	4.816088
269.305669	7999.919224	9.776512	-0.055306	4.816096
269.338924	7999.885649	9.781517	-0.055312	4.816086
269.303664	7999.854042	9.786522	-0.055305	4.816077
269.415899	7999.837916	9.791527	-0.055326	4.816072
269.359723	7999.973625	9.796531	-0.055316	4.816112
269.616421	7999.813776	9.801536	-0.055364	4.816064
269.517735	7999.894243	9.806541	-0.055346	4.816088
269.445706	7999.888675	9.811546	-0.055332	4.816086
269.563873	7999.899359	9.816551	-0.055354	4.816089
269.361909	7999.936304	9.821555	-0.055317	4.816101
269.257751	7999.888499	9.826560	-0.055297	4.816087
269.436806	7999.830855	9.831565	-0.055331	4.816069
269.338031	7999.892094	9.836570	-0.055312	4.816088
269.413919	7999.893470	9.841575	-0.055327	4.816088
269.509340	7999.913356	9.846579	-0.055344	4.816093
269.393675	7999.889909	9.851584	-0.055323	4.816087
269.581072	7999.963795	9.856589	-0.055358	4.816108
269.463067	7999.882627	9.861594	-0.055336	4.816084
269.595058	7999.895698	9.866599	-0.055361	4.816088
269.587522	7999.997038	9.871603	-0.055359	4.816117
269.644822	7999.815429	9.876608	-0.055370	4.816064
269.656571	7999.975864	9.881613	-0.055372	4.816111
269.735419	7999.880094	9.886618	-0.055387	4.816082
269.565438	8000.000931	9.891623	-0.055355	4.816118
269.566145	7999.872773	9.896627	-0.055355	4.816081
269.689495	7999.899573	9.901632	-0.055379	4.816088
269.518911	7999.900769	9.906637	-0.055347	4.816089
269.524495	7999.883785	9.911642	-0.055348	4.816084
269.801294	7999.879176	9.916647	-0.055399	4.816082
269.755230	7999.925347	9.921651	-0.055391	4.816095
269.832196	7999.888289	9.926656	-0.055405	4.816084
269.841381	7999.898073	9.931661	-0.055407	4.816087
269.734222	7999.891870	9.936666	-0.055387	4.816086
269.848773	7999.820243	9.941671	-0.055409	4.816064
269.730167	7999.985801	9.946675	-0.055387	4.816113
269.913084	7999.887638	9.951680	-0.055421	4.816084
269.703399	7999.899877	9.956685	-0.055382	4.816088
269.574613	7999.890079	9.961690	-0.055358	4.816086
269.783544	7999.904539	9.966695	-0.055397	4.816089
269.758272	7999.900883	9.971699	-0.055392	4.816088
269.697583	7999.836772	9.976704	-0.055381	4.816070
269.655254	7999.893691	9.981709	-0.055373	4.816087
269.714814	7999.911861	9.986714	-0.055384	4.816092
269.632595	7999.898631	9.991719	-0.055369	4.816088
269.400314	7999.884828	9.996723	-0.055326	4.816085
269.661914	7999.918397	10.001728	-0.055374	4.816094
269.805413	7999.892155	10.006733	-0.055401	4.816085
269.742265	7999.901700	10.011738	-0.055389	4.816089
270.044201	7999.900750	10.016743	-0.055446	4.816087
269.855870	7999.987076	10.021747	-0.055411	4.816113
269.867607	7999.829210	10.026752	-0.055413	4.816067
269.872641	7999.931846	10.031757	-0.055414	4.816097
269.986945	7999.863419	10.036762	-0.055435	4.816076
269.943441	7999.911772	10.041767	-0.055427	4.816090
269.742772	7999.893197	10.046771	-0.055390	4.816086
269.874153	7999.900916	10.051776	-0.055414	4.816088
269.860322	7999.922034	10.056781	-0.055412	4.816094
269.782455	7999.900337	10.061786	-0.055397	4.816088
269.701373	7999.921308	10.066791	-0.055382	4.816094
269.955081	8000.016688	10.071795	-0.055430	4.816121
270.014099	7999.883174	10.076800	-0.055441	4.816082
269.696200	8000.004543	10.081805	-0.055382	4.816119
269.792069	7999.881309	10.086810	-0.055399	4.816082
269.992077	7999.907357	10.091815	-0.055437	4.816089
269.872857	7999.889187	10.096819	-0.055415	4.816084
269.853465	7999.904863	10.101824	-0.055411	4.816089
269.890062	7999.911938	10.106829	-0.055418	4.816091
269.897560	8000.007142	10.111834	-0.055419	4.816118
269.937136	7999.896776	10.116839	-0.055427	4.816086
269.840381	7999.994369	10.121843	-0.055409	4.816115
269.867750	7999.906213	10.126848	-0.055414	4.816089
269.807135	7999.880556	10.131853	-0.055403	4.816082
269.858321	7999.926347	10.136858	-0.055412	4.816095
269.946466	7999.929012	10.141863	-0.055429	4.816095
269.905027	7999.896224	10.146867	-0.055421	4.816086
269.808762	7999.906239	10.151872	-0.055403	4.816089
269.890871	7999.814800	10.156877	-0.055418	4.816062
269.690441	8000.011993	10.161882	-0.055381	4.816121
269.659466	7999.826652	10.166887	-0.055375	4.816067
269.785338	7999.896222	10.171891	-0.055399	4.816087
269.874276	7999.829474	10.176896	-0.055416	4.816067
269.839110	7999.905748	10.181901	-0.055409	4.816089
269.741236	7999.889031	10.186906	-0.055391	4.816085
270.169407	7999.847637	10.191911	-0.055471	4.816070
270.080298	7999.901575	10.196915	-0.055454	4.816087
270.047081	7999.825142	10.201920	-0.055448	4.816064
270.106410	7999.931964	10.206925	-0.055459	4.816095
270.016563	7999.829941	10.211930	-0.055442	4.816066
270.004072	7999.909830	10.216935	-0.055440	4.816089
269.846871	7999.979628	10.221939	-0.055411	4.816111
269.843956	7999.816156	10.226944	-0.055410	4.816063
269.622648	7999.938202	10.231949	-0.055369	4.816100
269.870015	7999.809160	10.236954	-0.055415	4.816061
270.069059	7999.916369	10.241959	-0.055453	4.816091
269.931175	7999.886111	10.246963	-0.055427	4.816083
269.929092	7999.934144	10.251968	-0.055427	4.816097
269.929265	7999.913858	10.256973	-0.055427	4.816091
269.857602	7999.818573	10.261978	-0.055413	4.816064
269.888770	7999.954793	10.266983	-0.055419	4.816103
269.950658	7999.921735	10.271987	-0.055431	4.816093
270.086492	7999.862242	10.276992	-0.055456	4.816075
270.070547	7999.896139	10.281997	-0.055453	4.816085
270.113623	7999.990919	10.287002	-0.055461	4.816113
270.231636	8000.000533	10.292007	-0.055483	4.816115
269.959303	7999.887735	10.297011	-0.055433	4.816083
270.057235	7999.841443	10.302016	-0.055451	4.816069
270.029789	7999.934948	10.307021	-0.055446	4.816097
269.966581	7999.924198	10.312026	-0.055434	4.816094
270.104634	7999.896789	10.317031	-0.055460	4.816085
270.188880	7999.913270	10.322035	-0.055476	4.816089
270.155727	7999.811203	10.327040	-0.055469	4.816060
270.106946	7999.900049	10.332045	-0.055460	4.816086
270.144082	7999.910338	10.337050	-0.055467	4.816089
270.325663	7999.819628	10.342055	-0.055501	4.816061
270.247572	7999.989124	10.347059	-0.055487	4.816111
270.232959	7999.897005	10.352064	-0.055484	4.816084
270.130924	8000.028683	10.357069	-0.055465	4.816123
270.000809	7999.904569	10.362074	-0.055441	4.816088
270.211468	7999.926538	10.367079	-0.055480	4.816093
269.878049	7999.826524	10.372083	-0.055418	4.816066
269.825978	7999.904630	10.377088	-0.055409	4.816089
269.775944	7999.910139	10.382093	-0.055399	4.816091
269.720778	7999.839719	10.387098	-0.055389	4.816070
270.326427	7999.907277	10.392103	-0.055502	4.816087
270.107555	7999.894782	10.397107	-0.055461	4.816084
270.107462	7999.912943	10.402112	-0.055461	4.816090
270.052415	7999.808345	10.407117	-0.055451	4.816059
269.960564	8000.002159	10.412122	-0.055434	4.816117
270.030386	7999.828251	10.417127	-0.055447	4.816065
269.922520	7999.926711	10.422131	-0.055427	4.816095
270.035918	7999.817679	10.427136	-0.055448	4.816062
270.046084	7999.921476	10.432141	-0.055450	4.816093
270.028203	7999.894455	10.437146	-0.055447	4.816085
270.190706	8000.029845	10.442151	-0.055477	4.816123
270.106327	7999.892671	10.447155	-0.055461	4.816084
269.978727	7999.813466	10.452160	-0.055438	4.816061
270.075058	7999.932705	10.457165	-0.055456	4.816096
270.052626	7999.918419	10.462170	-0.055452	4.816092
270.015944	7999.836583	10.467175	-0.055445	4.816068
270.053118	7999.918437	10.472179	-0.055452	4.816092
270.197324	7999.832392	10.477184	-0.055479	4.816066
270.073475	7999.886771	10.482189	-0.055456	4.816082
269.857907	7999.880745	10.487194	-0.055416	4.816082
270.041419	7999.911836	10.492199	-0.055450	4.816090
270.037857	7999.888278	10.497203	-0.055449	4.816083
269.835110	7999.916664	10.502208	-0.055412	4.816092
270.014177	7999.893200	10.507213	-0.055445	4.816084
270.021097	7999.936055	10.512218	-0.055446	4.816097
270.180546	7999.836400	10.517223	-0.055476	4.816067
270.242120	7999.908014	10.522227	-0.055488	4.816088
270.477026	7999.948581	10.527232	-0.055531	4.816098
270.214768	7999.846646	10.532237	-0.055482	4.816070
269.942709	7999.820373	10.537242	-0.055432	4.816064
270.388053	7999.879694	10.542247	-0.055515	4.816079
270.165435	7999.904516	10.547251	-0.055473	4.816087
269.960185	7999.892268	10.552256	-0.055435	4.816084
269.820890	7999.883347	10.557261	-0.055409	4.816083
270.026872	7999.916981	10.562266	-0.055448	4.816091
270.263889	7999.833681	10.567271	-0.055492	4.816066
269.884734	7999.821496	10.572275	-0.055421	4.816064
270.071603	7999.918872	10.577280	-0.055456	4.816092
270.310319	7999.918917	10.582285	-0.055501	4.816090
270.046968	7999.814827	10.587290	-0.055452	4.816061
270.110197	7999.982604	10.592295	-0.055464	4.816110
270.024998	7999.810168	10.597299	-0.055448	4.816060
269.857374	7999.946001	10.602304	-0.055417	4.816101
270.201098	7999.907354	10.607309	-0.055481	4.816088
270.353575	7999.905842	10.612314	-0.055509	4.816086
270.320377	7999.921269	10.617319	-0.055503	4.816091
269.642359	7999.824642	10.622323	-0.055377	4.816066
269.509490	7999.963239	10.627328	-0.055352	4.816108
269.984582	7999.891717	10.632333	-0.055441	4.816084
270.251209	7999.918970	10.637338	-0.055490	4.816091
270.327158	7999.843441	10.642343	-0.055505	4.816068
270.428821	7999.906167	10.647347	-0.055524	4.816086
270.487240	7999.906159	10.652352	-0.055534	4.816086
270.380804	7999.910649	10.657357	-0.055515	4.816088
270.247265	7999.896492	10.662362	-0.055490	4.816084
270.107963	7999.912138	10.667367	-0.055464	4.816089
270.070551	7999.896513	10.672371	-0.055457	4.816085
270.195521	7999.901980	10.677376	-0.055480	4.816086
270.224084	7999.824527	10.682381	-0.055486	4.816063
270.060947	7999.905967	10.687386	-0.055455	4.816088
270.313034	7999.828280	10.692391	-0.055502	4.816064
270.450972	7999.931182	10.697395	-0.055528	4.816093
270.512475	7999.873550	10.702400	-0.055540	4.816076
270.526311	7999.864192	10.707405	-0.055542	4.816073
270.257482	7999.828363	10.712410	-0.055492	4.816064
270.521515	7999.937817	10.717415	-0.055541	4.816095
270.412070	7999.911276	10.722419	-0.055521	4.816088
270.281787	7999.820272	10.727424	-0.055497	4.816062
270.392409	7999.898113	10.732429	-0.055518	4.816084
270.257789	7999.990750	10.737434	-0.055493	4.816112
270.471172	7999.833321	10.742439	-0.055532	4.816064
270.320389	7999.903235	10.747443	-0.055504	4.816086
270.317613	7999.909598	10.752448	-0.055504	4.816088
270.319234	7999.834863	10.757453	-0.055504	4.816066
270.438606	7999.920339	10.762458	-0.055526	4.816090
270.576139	7999.929238	10.767463	-0.055552	4.816092
270.250055	7999.896647	10.772467	-0.055491	4.816084
270.261927	7999.909684	10.777472	-0.055494	4.816088
270.475647	7999.932778	10.782477	-0.055534	4.816094
270.349343	7999.895251	10.787482	-0.055510	4.816083
270.338513	7999.844858	10.792487	-0.055508	4.816069
270.312822	7999.826240	10.797491	-0.055503	4.816063
270.293636	7999.925235	10.802496	-0.055500	4.816092
270.352942	7999.918835	10.807501	-0.055511	4.816090
270.353796	7999.861175	10.812506	-0.055511	4.816073
270.658356	7999.866683	10.817511	-0.055568	4.816073
270.322695	7999.995209	10.822515	-0.055506	4.816113
270.468024	7999.917729	10.827520	-0.055533	4.816089
270.574536	7999.837411	10.832525	-0.055552	4.816065
270.362149	7999.917962	10.837530	-0.055513	4.816090
270.602164	7999.838988	10.842535	-0.055558	4.816065
270.456014	7999.999778	10.847539	-0.055531	4.816113
270.763429	7999.908137	10.852544	-0.055588	4.816085
270.640582	7999.818334	10.857549	-0.055565	4.816059
270.460526	7999.913354	10.862554	-0.055532	4.816088
270.510363	7999.872602	10.867559	-0.055541	4.816076
270.472798	7999.923199	10.872563	-0.055534	4.816091
270.422617	7999.858208	10.877568	-0.055525	4.816072
270.559226	7999.861750	10.882573	-0.055550	4.816072
270.577130	7999.835374	10.887578	-0.055553	4.816064
270.540737	7999.873175	10.892583	-0.055547	4.816076
270.431658	7999.884026	10.897587	-0.055527	4.816079
270.405964	7999.851523	10.902592	-0.055522	4.816070
270.357007	7999.960661	10.907597	-0.055513	4.816102
270.497145	7999.824340	10.912602	-0.055539	4.816062
270.460826	7999.878164	10.917607	-0.055532	4.816078
270.028727	7999.909882	10.922611	-0.055452	4.816089
270.294265	7999.941388	10.927616	-0.055501	4.816097
270.577459	7999.846105	10.932621	-0.055554	4.816068
270.593616	7999.944671	10.937626	-0.055557	4.816096
270.515959	7999.878116	10.942631	-0.055543	4.816077
270.552017	7999.852068	10.947635	-0.055549	4.816069
270.550847	7999.901187	10.952640	-0.055549	4.816084
270.510239	7999.870550	10.957645	-0.055542	4.816075
270.402096	7999.853646	10.962650	-0.055522	4.816071
270.794905	7999.862885	10.967655	-0.055595	4.816071
270.430132	7999.925728	10.972659	-0.055527	4.816092
270.433785	7999.861710	10.977664	-0.055528	4.816073
270.787198	7999.869169	10.982669	-0.055594	4.816073
270.657577	7999.910626	10.987674	-0.055569	4.816086
270.637923	7999.821619	10.992679	-0.055566	4.816060
270.540757	7999.969409	10.997683	-0.055548	4.816104
270.477795	7999.843303	11.002688	-0.055536	4.816067
270.707698	7999.868825	11.007693	-0.055579	4.816074
270.668090	7999.926862	11.012698	-0.055572	4.816091
270.848238	7999.856420	11.017703	-0.055605	4.816069
270.836087	7999.869023	11.022707	-0.055603	4.816073
270.696624	7999.863303	11.027712	-0.055577	4.816072
270.639127	7999.867610	11.032717	-0.055566	4.816074
270.386696	7999.869462	11.037722	-0.055520	4.816075
270.459517	7999.909236	11.042727	-0.055533	4.816087
270.252934	7999.955710	11.047731	-0.055495	4.816101
270.760057	7999.856996	11.052736	-0.055589	4.816070
270.686214	7999.868484	11.057741	-0.055575	4.816074
270.471970	7999.843255	11.062746	-0.055536	4.816067
270.609957	7999.947227	11.067751	-0.055561	4.816097
270.550053	7999.898083	11.072755	-0.055550	4.816083
270.418853	7999.874354	11.077760	-0.055526	4.816077
270.648958	7999.879585	11.082765	-0.055569	4.816077
270.681896	7999.847072	11.087770	-0.055575	4.816067
270.526476	7999.894471	11.092775	-0.055546	4.816082
270.621581	7999.824629	11.097779	-0.055564	4.816061
270.815209	7999.922130	11.102784	-0.055600	4.816089
270.731669	7999.867217	11.107789	-0.055584	4.816073
270.524656	7999.924366	11.112794	-0.055546	4.816091
270.743395	7999.883461	11.117799	-0.055587	4.816078
270.830724	7999.849795	11.122803	-0.055603	4.816067
270.668092	7999.846861	11.127808	-0.055573	4.816067
270.802965	7999.859985	11.132813	-0.055598	4.816070
270.885149	7999.934109	11.137818	-0.055613	4.816092
270.834043	7999.848806	11.142823	-0.055604	4.816067
270.640484	7999.864540	11.147827	-0.055568	4.816073
270.676116	7999.840621	11.152832	-0.055575	4.816065
270.918829	7999.926192	11.157837	-0.055620	4.816089
270.487004	7999.917324	11.162842	-0.055539	4.816089
270.772855	7999.871224	11.167847	-0.055593	4.816074
270.962273	7999.951559	11.172851	-0.055628	4.816096
270.801348	7999.827954	11.177856	-0.055598	4.816061
270.904732	7999.847986	11.182861	-0.055617	4.816066
270.925192	7999.914586	11.187866	-0.055621	4.816086
270.812147	7999.816414	11.192871	-0.055600	4.816058
270.864317	7999.925245	11.197875	-0.055610	4.816089
270.722630	7999.828692	11.202880	-0.055584	4.816062
270.840719	7999.936578	11.207885	-0.055606	4.816093
270.574475	7999.813206	11.212890	-0.055556	4.816058
270.620040	7999.930463	11.217895	-0.055565	4.816092
270.748505	7999.835587	11.222899	-0.055589	4.816064
270.706584	7999.933104	11.227904	-0.055581	4.816092
270.737773	7999.823653	11.232909	-0.055587	4.816060
270.780138	7999.829764	11.237914	-0.055595	4.816062
270.768829	7999.938516	11.242919	-0.055593	4.816094
270.896572	7999.817992	11.247923	-0.055616	4.816058
270.911187	7999.848169	11.252928	-0.055619	4.816066
271.041599	7999.863349	11.257933	-0.055644	4.816070
270.882784	7999.937391	11.262938	-0.055614	4.816093
271.124917	7999.859523	11.267943	-0.055659	4.816069
271.096292	7999.818421	11.272947	-0.055654	4.816057
270.900705	7999.927047	11.277952	-0.055618	4.816089
270.940053	7999.851924	11.282957	-0.055625	4.816067
270.794340	7999.827933	11.287962	-0.055598	4.816061
270.971060	7999.846085	11.292967	-0.055631	4.816065
271.024764	7999.838515	11.297971	-0.055641	4.816063
270.910398	7999.930451	11.302976	-0.055620	4.816090
270.940397	7999.869045	11.307981	-0.055625	4.816072
270.905433	7999.820351	11.312986	-0.055619	4.816058
270.786007	7999.883355	11.317991	-0.055597	4.816077
270.783837	7999.866230	11.322995	-0.055596	4.816072
270.883741	7999.922516	11.328000	-0.055615	4.816088
270.730985	7999.867421	11.333005	-0.055587	4.816073
270.642029	7999.825228	11.338010	-0.055570	4.816061
270.906609	7999.950716	11.343015	-0.055619	4.816096
270.897867	7999.842679	11.348019	-0.055618	4.816065
270.779609	7999.819183	11.353024	-0.055596	4.816059
270.861142	7999.929613	11.358029	-0.055611	4.816090
270.808371	7999.818645	11.363034	-0.055601	4.816058
270.573114	7999.921213	11.368039	-0.055558	4.816089
270.930015	7999.860374	11.373043	-0.055624	4.816070
270.917130	7999.820624	11.378048	-0.055622	4.816058
270.867784	7999.921212	11.383053	-0.055613	4.816088
270.715489	7999.809513	11.388058	-0.055584	4.816056
270.774133	7999.917393	11.393063	-0.055595	4.816087
270.806247	7999.903024	11.398067	-0.055601	4.816083
270.802105	7999.917908	11.403072	-0.055600	4.816087
271.140402	7999.820415	11.408077	-0.055663	4.816057
270.789644	7999.920897	11.413082	-0.055598	4.816088
270.992377	7999.842317	11.418087	-0.055636	4.816064
270.894238	7999.856571	11.423091	-0.055618	4.816069
270.663686	7999.917567	11.428096	-0.055575	4.816088
270.909590	7999.824813	11.433101	-0.055621	4.816059
270.772606	7999.994316	11.438106	-0.055595	4.816110
270.970638	7999.821654	11.443111	-0.055632	4.816058
270.948858	7999.913126	11.448115	-0.055628	4.816085
270.906761	7999.821577	11.453120	-0.055620	4.816059
271.190610	7999.830984	11.458125	-0.055673	4.816060
271.028947	7999.887884	11.463130	-0.055643	4.816077
270.812264	7999.930972	11.468135	-0.055603	4.816091
270.865657	7999.825126	11.473139	-0.055613	4.816060
270.725633	7999.912325	11.478144	-0.055587	4.816086
270.896927	7999.916494	11.483149	-0.055619	4.816086
270.875341	7999.892609	11.488154	-0.055615	4.816079
270.930396	7999.835928	11.493159	-0.055625	4.816063
270.863902	7999.820845	11.498163	-0.055613	4.816059
270.940746	7999.916237	11.503168	-0.055627	4.816086
270.989412	7999.880804	11.508173	-0.055636	4.816075
271.184833	7999.855500	11.513178	-0.055673	4.816067
271.151961	7999.920069	11.518183	-0.055667	4.816086
271.099212	7999.817645	11.523187	-0.055657	4.816056
270.959177	7999.937957	11.528192	-0.055631	4.816092
271.031421	7999.873042	11.533197	-0.055644	4.816073
270.761711	7999.811560	11.538202	-0.055594	4.816056
271.017471	7999.942229	11.543207	-0.055642	4.816093
270.903048	7999.825873	11.548211	-0.055621	4.816060
270.888390	7999.821341	11.553216	-0.055618	4.816059
270.994420	7999.848897	11.558221	-0.055638	4.816066
270.969755	7999.918955	11.563226	-0.055633	4.816087
271.011071	7999.835322	11.568231	-0.055641	4.816062
271.091859	7999.851741	11.573235	-0.055656	4.816066
271.248179	7999.844957	11.578240	-0.055685	4.816064
271.372325	7999.838661	11.583245	-0.055708	4.816061
271.086981	7999.902939	11.588250	-0.055655	4.816081
271.131842	7999.832188	11.593255	-0.055664	4.816060
271.013497	7999.915506	11.598259	-0.055642	4.816085
270.962957	7999.833418	11.603264	-0.055632	4.816062
271.146061	7999.868776	11.608269	-0.055667	4.816071
271.046152	7999.924656	11.613274	-0.055648	4.816088
271.105054	7999.824250	11.618279	-0.055659	4.816058
271.136154	7999.912406	11.623283	-0.055665	4.816084
271.166266	7999.804003	11.628288	-0.055670	4.816052
271.033206	7999.907351	11.633293	-0.055646	4.816083
270.820931	7999.821271	11.638298	-0.055606	4.816059
271.084647	7999.857018	11.643303	-0.055655	4.816068
271.158620	7999.949154	11.648307	-0.055669	4.816094
271.163089	7999.839219	11.653312	-0.055670	4.816062
271.210737	7999.869993	11.658317	-0.055679	4.816071
271.133121	7999.814119	11.663322	-0.055665	4.816055
271.052803	7999.886375	11.668327	-0.055650	4.816077
270.984116	7999.854162	11.673331	-0.055637	4.816068
271.137921	7999.929582	11.678336	-0.055666	4.816089
271.130493	7999.850408	11.683341	-0.055664	4.816066
271.172614	7999.813789	11.688346	-0.055672	4.816055
271.139327	7999.832419	11.693351	-0.055666	4.816060
271.191508	7999.923092	11.698355	-0.055676	4.816087
270.988963	7999.833983	11.703360	-0.055638	4.816062
271.038146	7999.823127	11.708365	-0.055647	4.816058
270.941819	7999.918593	11.713370	-0.055630	4.816087
270.925513	7999.838192	11.718375	-0.055627	4.816063
270.951501	7999.822644	11.723379	-0.055631	4.816059
270.980244	8000.000483	11.728384	-0.055637	4.816110
271.173965	7999.839492	11.733389	-0.055673	4.816062
271.137728	7999.817479	11.738394	-0.055666	4.816056
270.931217	7999.933385	11.743399	-0.055628	4.816091
271.385681	7999.819833	11.748403	-0.055712	4.816055
271.110741	7999.913140	11.753408	-0.055661	4.816084
271.125909	7999.845056	11.758413	-0.055664	4.816064
271.148963	7999.896749	11.763418	-0.055669	4.816079
271.125817	7999.899540	11.768423	-0.055664	4.816080
270.951910	7999.899606	11.773427	-0.055632	4.816081
270.893739	7999.909241	11.778432	-0.055621	4.816084
270.890835	7999.854718	11.783437	-0.055621	4.816068
270.860519	7999.832812	11.788442	-0.055615	4.816062
270.888296	7999.927316	11.793447	-0.055620	4.816089
271.178395	7999.805453	11.798451	-0.055674	4.816052
271.167741	7999.899263	11.803456	-0.055673	4.816080
270.998489	7999.931458	11.808461	-0.055641	4.816090
271.141935	7999.800536	11.813466	-0.055668	4.816051
271.039657	7999.904440	11.818471	-0.055649	4.816082
271.058534	7999.839628	11.823475	-0.055652	4.816063
271.065754	7999.916671	11.828480	-0.055654	4.816085
271.224690	7999.851186	11.833485	-0.055683	4.816065
270.946549	7999.923071	11.838490	-0.055632	4.816088
271.147531	7999.843392	11.843495	-0.055669	4.816064
271.422503	7999.829140	11.848499	-0.055720	4.816058
271.179721	7999.933709	11.853504	-0.055675	4.816090
271.331853	7999.836056	11.858509	-0.055704	4.816060
271.356636	7999.895258	11.863514	-0.055708	4.816078
271.253403	7999.830375	11.868519	-0.055689	4.816059
271.215823	7999.817951	11.873523	-0.055682	4.816056
271.171978	7999.896207	11.878528	-0.055674	4.816079
271.112827	7999.871644	11.883533	-0.055663	4.816072
271.022876	7999.956544	11.888538	-0.055646	4.816097
271.097080	7999.885255	11.893543	-0.055660	4.816076
271.266618	7999.904346	11.898547	-0.055692	4.816081
271.034509	7999.841407	11.903552	-0.055649	4.816064
271.144962	7999.840203	11.908557	-0.055669	4.816063
271.272305	7999.819010	11.913562	-0.055693	4.816056
271.307395	7999.920057	11.918567	-0.055700	4.816085
271.346993	7999.825711	11.923571	-0.055707	4.816057
271.063745	7999.897504	11.928576	-0.055654	4.816080
271.427146	7999.835714	11.933581	-0.055722	4.816060
271.353556	7999.924115	11.938586	-0.055708	4.816086
271.202541	7999.835937	11.943591	-0.055680	4.816061
271.159594	7999.912073	11.948595	-0.055672	4.816084
271.079478	7999.889267	11.953600	-0.055658	4.816077
271.167559	7999.827842	11.958605	-0.055674	4.816059
271.208266	7999.821105	11.963610	-0.055682	4.816057
271.085143	7999.937451	11.968615	-0.055659	4.816091
271.127813	7999.826070	11.973619	-0.055667	4.816059
271.187506	7999.933970	11.978624	-0.055678	4.816090
271.364685	7999.835701	11.983629	-0.055711	4.816060
271.031431	7999.905522	11.988634	-0.055649	4.816082
271.053863	7999.842911	11.993639	-0.055653	4.816064
271.479298	7999.849537	11.998643	-0.055732	4.816064
271.408994	7999.807681	12.003648	-0.055719	4.816052
271.251752	7999.926614	12.008653	-0.055690	4.816087
271.311110	7999.800580	12.013658	-0.055701	4.816050
271.321115	7999.897969	12.018663	-0.055703	4.816079
271.325153	7999.828616	12.023667	-0.055704	4.816058
271.295544	7999.814200	12.028672	-0.055698	4.816054
271.443156	7999.840372	12.033677	-0.055726	4.816061
271.508982	7999.902452	12.038682	-0.055738	4.816079
271.410554	7999.819497	12.043687	-0.055720	4.816055
271.382491	7999.917266	12.048691	-0.055715	4.816084
271.392143	7999.815969	12.053696	-0.055717	4.816054
271.353672	7999.833438	12.058701	-0.055710	4.816059
271.321122	7999.918307	12.063706	-0.055704	4.816084
271.492306	7999.826340	12.068711	-0.055736	4.816057
271.297879	7999.828171	12.073715	-0.055699	4.816058
271.160535	7999.905806	12.078720	-0.055674	4.816082
271.432169	7999.917129	12.083725	-0.055725	4.816084
271.341061	7999.823625	12.088730	-0.055708	4.816057
271.304147	7999.837917	12.093735	-0.055701	4.816061
271.336650	7999.854532	12.098739	-0.055707	4.816066
271.363525	7999.914840	12.103744	-0.055712	4.816083
271.328883	7999.841583	12.108749	-0.055705	4.816062
271.195430	7999.825289	12.113754	-0.055681	4.816058
271.096101	7999.835249	12.118759	-0.055662	4.816061
271.129057	7999.931984	12.123763	-0.055668	4.816089
270.908572	7999.908777	12.128768	-0.055627	4.816084
271.158833	7999.828920	12.133773	-0.055674	4.816059
271.279323	7999.909078	12.138778	-0.055697	4.816082
271.227724	7999.919900	12.143783	-0.055687	4.816085
271.250134	7999.818835	12.148787	-0.055691	4.816056
271.236767	7999.901915	12.153792	-0.055689	4.816080
271.295280	7999.837819	12.158797	-0.055700	4.816061
271.323371	7999.812695	12.163802	-0.055705	4.816054
271.253423	7999.923593	12.168807	-0.055692	4.816086
271.481552	7999.834791	12.173811	-0.055735	4.816059
271.286421	7999.843019	12.178816	-0.055698	4.816063
271.383144	7999.857590	12.183821	-0.055716	4.816066
271.234815	7999.839959	12.188826	-0.055689	4.816062
271.170021	7999.960564	12.193831	-0.055677	4.816098
271.148270	7999.819178	12.198835	-0.055673	4.816056
271.130532	7999.818862	12.203840	-0.055669	4.816056
271.308506	7999.920355	12.208845	-0.055703	4.816085
271.280974	7999.911316	12.213850	-0.055698	4.816083
271.425749	7999.812462	12.218855	-0.055725	4.816053
271.465636	7999.822801	12.223859	-0.055732	4.816056
271.254683	7999.920469	12.228864	-0.055693	4.816085
271.435930	7999.850046	12.233869	-0.055727	4.816064
271.479047	7999.910648	12.238874	-0.055735	4.816081
271.233092	7999.986320	12.243879	-0.055689	4.816105
271.352332	7999.907299	12.248883	-0.055711	4.816081
271.453014	7999.898442	12.253888	-0.055730	4.816078
271.537645	7999.834818	12.258893	-0.055746	4.816059
271.509806	7999.808684	12.263898	-0.055741	4.816051
271.300724	7999.985430	12.268903	-0.055702	4.816104
271.312992	7999.817954	12.273907	-0.055704	4.816055
271.223060	7999.897514	12.278912	-0.055687	4.816079
271.279409	7999.807743	12.283917	-0.055698	4.816052
271.284283	7999.933880	12.288922	-0.055699	4.816089
271.268371	7999.928256	12.293927	-0.055696	4.816088
271.372200	7999.806230	12.298931	-0.055715	4.816051
271.335537	7999.905980	12.303936	-0.055709	4.816081
271.489664	7999.844681	12.308941	-0.055737	4.816062
271.316894	7999.811654	12.313946	-0.055705	4.816053
271.329522	7999.915499	12.318951	-0.055708	4.816084
271.544331	7999.829661	12.323955	-0.055748	4.816057
271.153171	7999.909116	12.328960	-0.055675	4.816083
271.207604	7999.827857	12.333965	-0.055685	4.816059
271.332440	7999.834390	12.338970	-0.055708	4.816060
271.356841	7999.823086	12.343975	-0.055713	4.816056
271.413116	7999.934130	12.348979	-0.055724	4.816089
271.400445	7999.818543	12.353984	-0.055721	4.816055
271.567072	7999.905945	12.358989	-0.055752	4.816079
271.226976	7999.797259	12.363994	-0.055689	4.816049
271.389430	7999.916630	12.368999	-0.055719	4.816084
271.501185	7999.812906	12.374003	-0.055740	4.816053
271.455784	7999.901816	12.379008	-0.055732	4.816079
271.540823	7999.878790	12.384013	-0.055748	4.816072
271.498400	7999.850256	12.389018	-0.055740	4.816064
271.323740	7999.915466	12.394023	-0.055707	4.816084
271.476542	7999.918233	12.399027	-0.055736	4.816084
271.506897	7999.807697	12.404032	-0.055742	4.816051
271.482251	7999.835029	12.409037	-0.055737	4.816059
271.374879	7999.904660	12.414042	-0.055717	4.816080
271.368761	7999.892804	12.419047	-0.055716	4.816077
271.533351	7999.843444	12.424051	-0.055747	4.816061
271.303948	7999.890574	12.429056	-0.055704	4.816076
271.228192	7999.827256	12.434061	-0.055690	4.816058
271.245714	7999.894872	12.439066	-0.055693	4.816078
271.323647	7999.911240	12.444071	-0.055708	4.816082
271.468762	7999.842300	12.449075	-0.055735	4.816061
271.173126	7999.882893	12.454080	-0.055680	4.816075
271.564318	7999.845106	12.459085	-0.055753	4.816062
271.456590	7999.911526	12.464090	-0.055733	4.816082
271.419290	7999.811517	12.469095	-0.055726	4.816053
271.557509	7999.834315	12.474099	-0.055752	4.816059
271.239534	7999.849936	12.479104	-0.055692	4.816065
271.380174	7999.847142	12.484109	-0.055719	4.816063
271.359049	7999.908718	12.489114	-0.055715	4.816081
271.481688	7999.891713	12.494119	-0.055738	4.816076
271.589371	7999.835983	12.499123	-0.055758	4.816059
271.551125	7999.826751	12.504128	-0.055751	4.816056
271.578756	7999.835801	12.509133	-0.055756	4.816059
271.461642	7999.829416	12.514138	-0.055734	4.816058
271.303011	7999.910939	12.519143	-0.055705	4.816082
271.502425	7999.852594	12.524147	-0.055742	4.816064
271.448341	7999.832394	12.529152	-0.055732	4.816059
271.555175	7999.847148	12.534157	-0.055752	4.816062
271.528295	7999.936394	12.539162	-0.055747	4.816089
271.474970	7999.826481	12.544167	-0.055737	4.816057
271.424284	7999.845865	12.549171	-0.055728	4.816063
271.213372	7999.827103	12.554176	-0.055688	4.816058
271.478131	7999.908802	12.559181	-0.055738	4.816081
271.634945	7999.805892	12.564186	-0.055767	4.816050
271.626675	7999.914701	12.569191	-0.055766	4.816082
271.666738	7999.852408	12.574195	-0.055773	4.816063
271.436070	7999.841834	12.579200	-0.055730	4.816061
271.323810	7999.833401	12.584205	-0.055709	4.816059
271.096656	7999.919026	12.589210	-0.055667	4.816086
271.456479	7999.831536	12.594215	-0.055734	4.816058
271.579252	7999.835896	12.599219	-0.055757	4.816059
271.539955	7999.902485	12.604224	-0.055750	4.816079
271.506053	7999.834582	12.609229	-0.055743	4.816059
271.481149	7999.928136	12.614234	-0.055739	4.816086
271.382373	7999.824879	12.619239	-0.055720	4.816057
271.556447	7999.850462	12.624243	-0.055753	4.816063
271.525030	7999.836013	12.629248	-0.055747	4.816059
271.607764	7999.925103	12.634253	-0.055763	4.816085
271.573327	7999.808055	12.639258	-0.055756	4.816051
271.696565	7999.926718	12.644263	-0.055779	4.816085
271.671061	7999.847217	12.649267	-0.055775	4.816062
271.753267	7999.802776	12.654272	-0.055790	4.816048
271.625780	7999.908362	12.659277	-0.055766	4.816080
271.600819	7999.898302	12.664282	-0.055762	4.816077
271.624711	7999.792990	12.669287	-0.055766	4.816046
271.634476	7999.913875	12.674291	-0.055768	4.816081
271.593086	7999.889631	12.679296	-0.055760	4.816074
271.620578	7999.840997	12.684301	-0.055765	4.816060
271.738071	7999.842058	12.689306	-0.055787	4.816060
271.520085	7999.830645	12.694311	-0.055747	4.816058
271.487756	7999.874928	12.699315	-0.055741	4.816071
271.470657	7999.819079	12.704320	-0.055738	4.816054
271.476680	7999.931351	12.709325	-0.055739	4.816087
271.563470	7999.834653	12.714330	-0.055755	4.816059
271.486142	7999.831123	12.719335	-0.055741	4.816058
271.712313	7999.829876	12.724339	-0.055783	4.816056
271.588442	7999.913095	12.729344	-0.055760	4.816081
271.588745	7999.847947	12.734349	-0.055760	4.816062
271.583941	7999.805138	12.739354	-0.055759	4.816050
271.806520	7999.924530	12.744359	-0.055801	4.816084
271.798160	7999.849611	12.749363	-0.055799	4.816062
271.682001	7999.825084	12.754368	-0.055778	4.816055
271.673597	7999.860186	12.759373	-0.055776	4.816065
271.554231	7999.928533	12.764378	-0.055754	4.816086
271.452071	7999.856191	12.769383	-0.055735	4.816065
271.723915	7999.852565	12.774387	-0.055786	4.816063
271.680523	7999.824013	12.779392	-0.055778	4.816055
271.470123	7999.838373	12.784397	-0.055738	4.816060
271.355413	7999.946326	12.789402	-0.055717	4.816092
271.504390	7999.836866	12.794407	-0.055745	4.816059
271.470507	7999.860826	12.799411	-0.055739	4.816067
271.402086	7999.820072	12.804416	-0.055726	4.816055
271.147718	7999.956477	12.809421	-0.055679	4.816096
271.361408	7999.875959	12.814426	-0.055719	4.816072
271.347046	7999.876772	12.819431	-0.055716	4.816072
271.220561	7999.890513	12.824435	-0.055692	4.816077
271.134454	7999.895371	12.829440	-0.055676	4.816079
271.232303	7999.887531	12.834445	-0.055695	4.816076
271.437637	7999.851725	12.839450	-0.055733	4.816064
271.575646	7999.919383	12.844455	-0.055759	4.816083
271.420131	7999.836464	12.849459	-0.055730	4.816060
271.389358	7999.832708	12.854464	-0.055724	4.816059
271.376044	7999.855972	12.859469	-0.055722	4.816066
271.358837	7999.928301	12.864474	-0.055719	4.816087
271.168912	7999.834079	12.869479	-0.055683	4.816060
271.435228	7999.875215	12.874483	-0.055733	4.816071
271.259045	7999.859217	12.879488	-0.055700	4.816067
271.260787	7999.974615	12.884493	-0.055701	4.816101
271.462550	7999.851155	12.889498	-0.055738	4.816064
271.596539	7999.839696	12.894503	-0.055763	4.816060
271.499612	7999.851835	12.899507	-0.055745	4.816064
271.452975	7999.814679	12.904512	-0.055736	4.816053
271.517663	7999.842557	12.909517	-0.055749	4.816061
271.823496	7999.918590	12.914522	-0.055806	4.816082
271.677768	7999.824097	12.919527	-0.055778	4.816055
271.845753	7999.852775	12.924531	-0.055810	4.816062
271.533957	7999.817234	12.929536	-0.055752	4.816054
271.600961	7999.849427	12.934541	-0.055764	4.816063
271.568590	7999.830688	12.939546	-0.055758	4.816057
271.688621	7999.922590	12.944551	-0.055781	4.816084
271.820189	7999.869428	12.949555	-0.055805	4.816067
271.654967	7999.827991	12.954560	-0.055775	4.816056
271.710920	7999.858916	12.959565	-0.055785	4.816065
271.700439	7999.843777	12.964570	-0.055783	4.816060
271.520045	7999.833044	12.969575	-0.055750	4.816058
271.546632	7999.855961	12.974579	-0.055755	4.816065
271.742547	7999.936416	12.979584	-0.055791	4.816087
271.878414	7999.844878	12.984589	-0.055816	4.816060
271.765564	7999.848183	12.989594	-0.055795	4.816061
271.629544	7999.824365	12.994599	-0.055770	4.816055
271.755135	7999.854413	12.999603	-0.055794	4.816063
271.648092	7999.815097	13.004608	-0.055774	4.816052
271.659541	7999.859104	13.009613	-0.055776	4.816065
271.535897	7999.854737	13.014618	-0.055753	4.816064
271.276181	7999.857524	13.019623	-0.055705	4.816067
271.641797	7999.888706	13.024627	-0.055773	4.816074
271.567875	7999.922624	13.029632	-0.055759	4.816084
271.793178	7999.840180	13.034637	-0.055801	4.816059
271.702651	7999.850298	13.039642	-0.055784	4.816062
271.574879	7999.820221	13.044647	-0.055760	4.816054
271.714407	7999.843043	13.049651	-0.055787	4.816060
271.377706	7999.827348	13.054656	-0.055724	4.816057
271.385135	7999.941781	13.059661	-0.055725	4.816091
271.780548	7999.850662	13.064666	-0.055799	4.816062
271.629499	7999.846868	13.069671	-0.055771	4.816062
271.519403	7999.886541	13.074675	-0.055751	4.816074
271.616990	7999.833833	13.079680	-0.055769	4.816058
271.478642	7999.876201	13.084685	-0.055743	4.816071
271.559344	7999.864846	13.089690	-0.055758	4.816067
271.311498	7999.941552	13.094695	-0.055712	4.816091
271.497484	7999.842374	13.099699	-0.055747	4.816061
271.544504	7999.805843	13.104704	-0.055755	4.816050
271.482011	7999.830354	13.109709	-0.055744	4.816058
271.544591	7999.838967	13.114714	-0.055756	4.816060
271.574850	7999.920700	13.119719	-0.055761	4.816084
271.369921	7999.876410	13.124723	-0.055723	4.816072
271.557572	7999.862716	13.129728	-0.055758	4.816067
271.667637	7999.852961	13.134733	-0.055779	4.816063
271.899235	7999.843266	13.139738	-0.055822	4.816059
271.766684	7999.823784	13.144743	-0.055797	4.816054
271.757542	7999.844987	13.149747	-0.055796	4.816060
271.649216	7999.925283	13.154752	-0.055775	4.816084
271.592636	7999.832402	13.159757	-0.055765	4.816058
271.676548	7999.831787	13.164762	-0.055781	4.816057
271.963676	7999.914960	13.169767	-0.055834	4.816080
271.596945	7999.848517	13.174771	-0.055766	4.816062
271.563444	7999.830825	13.179776	-0.055760	4.816057
271.732500	7999.868067	13.184781	-0.055791	4.816067
271.614533	7999.880894	13.189786	-0.055769	4.816072
271.616413	7999.859569	13.194791	-0.055770	4.816065
271.566225	7999.908871	13.199795	-0.055760	4.816080
271.648891	7999.867643	13.204800	-0.055776	4.816068
271.771874	7999.939303	13.209805	-0.055799	4.816088
271.575066	7999.865250	13.214810	-0.055762	4.816067
271.472773	7999.861269	13.219815	-0.055743	4.816067
271.721200	7999.901015	13.224819	-0.055790	4.816077
271.780469	7999.830523	13.229824	-0.055801	4.816056
271.692988	7999.860992	13.234829	-0.055784	4.816065
271.748795	7999.873756	13.239834	-0.055795	4.816069
271.579543	7999.846133	13.244839	-0.055763	4.816062
271.385123	7999.883213	13.249843	-0.055727	4.816074
271.452319	7999.890842	13.254848	-0.055740	4.816075
271.480900	7999.875341	13.259853	-0.055745	4.816071
271.297749	7999.889126	13.264858	-0.055711	4.816076
271.155053	7999.976277	13.269863	-0.055685	4.816102
271.397305	7999.886662	13.274867	-0.055730	4.816074
271.386378	7999.871515	13.279872	-0.055728	4.816070
271.460830	7999.924138	13.284877	-0.055742	4.816085
271.515847	7999.870660	13.289882	-0.055752	4.816069
271.502678	7999.867223	13.294887	-0.055750	4.816068
271.758610	7999.881468	13.299891	-0.055797	4.816071
271.697797	7999.867555	13.304896	-0.055786	4.816067
271.800372	7999.849119	13.309901	-0.055805	4.816061
271.511424	7999.835355	13.314906	-0.055751	4.816059
271.700767	7999.914623	13.319911	-0.055787	4.816081
271.674496	7999.859676	13.324915	-0.055782	4.816065
271.658872	7999.846580	13.329920	-0.055779	4.816061
271.715697	7999.867907	13.334925	-0.055790	4.816067
271.611854	7999.842535	13.339930	-0.055770	4.816060
271.567026	7999.962433	13.344935	-0.055762	4.816096
271.538479	7999.898900	13.349939	-0.055757	4.816077
271.609589	7999.851054	13.354944	-0.055770	4.816063
271.412853	7999.853911	13.359949	-0.055733	4.816065
271.669031	7999.872433	13.364954	-0.055781	4.816069
271.626031	7999.828934	13.369959	-0.055773	4.816056
271.592486	7999.868923	13.374963	-0.055767	4.816068
271.682367	7999.832098	13.379968	-0.055784	4.816057
271.826042	7999.972496	13.384973	-0.055811	4.816097
271.628699	7999.856774	13.389978	-0.055774	4.816064
271.659829	7999.831705	13.394983	-0.055780	4.816057
271.668082	7999.875654	13.399987	-0.055781	4.816070
271.661949	7999.838162	13.404992	-0.055780	4.816059
271.476870	7999.930957	13.409997	-0.055746	4.816087
271.532902	7999.902066	13.415002	-0.055756	4.816078
271.633464	7999.837661	13.420007	-0.055775	4.816059
271.962035	7999.876720	13.425011	-0.055836	4.816069
271.859505	7999.842826	13.430016	-0.055817	4.816059
272.017712	7999.843554	13.435021	-0.055847	4.816059
271.998076	7999.846409	13.440026	-0.055843	4.816059
271.615018	7999.864056	13.445031	-0.055772	4.816067
271.791618	7999.931345	13.450035	-0.055805	4.816085
271.742223	7999.806548	13.455040	-0.055796	4.816049
271.738234	7999.844935	13.460045	-0.055795	4.816060
271.643983	7999.885963	13.465050	-0.055778	4.816073
271.482433	7999.955683	13.470055	-0.055748	4.816094
271.801300	7999.893089	13.475059	-0.055807	4.816074
271.764857	7999.862526	13.480064	-0.055800	4.816065
271.865217	7999.863277	13.485069	-0.055819	4.816065
271.994914	7999.865627	13.490074	-0.055843	4.816065
271.601920	7999.855322	13.495079	-0.055770	4.816064
271.859834	7999.871739	13.500083	-0.055818	4.816068
271.906020	7999.923852	13.505088	-0.055827	4.816083
271.881916	7999.848648	13.510093	-0.055822	4.816061
271.723015	7999.872485	13.515098	-0.055793	4.816069
271.854527	7999.827867	13.520103	-0.055817	4.816055
272.172387	7999.843233	13.525107	-0.055876	4.816058
272.039881	7999.915615	13.530112	-0.055852	4.816079
271.882485	7999.854023	13.535117	-0.055823	4.816062
272.082213	7999.848026	13.540122	-0.055860	4.816059
271.862861	7999.837656	13.545127	-0.055819	4.816058
271.988180	7999.855949	13.550131	-0.055842	4.816062
272.232550	7999.834735	13.555136	-0.055888	4.816055
271.967332	7999.874809	13.560141	-0.055839	4.816068
271.679013	7999.883487	13.565146	-0.055785	4.816072
271.829551	7999.844555	13.570151	-0.055813	4.816060
271.965894	7999.871593	13.575155	-0.055839	4.816067
271.832692	7999.851030	13.580160	-0.055814	4.816062
271.792803	7999.862064	13.585165	-0.055806	4.816065
271.905636	7999.869449	13.590170	-0.055827	4.816067
271.641728	7999.864683	13.595175	-0.055778	4.816067
271.633496	7999.895516	13.600179	-0.055777	4.816076
271.643362	7999.942699	13.605184	-0.055779	4.816089
271.699116	7999.933030	13.610189	-0.055789	4.816086
271.699315	7999.860402	13.615194	-0.055789	4.816065
271.685263	7999.832380	13.620199	-0.055787	4.816057
271.896233	7999.870381	13.625203	-0.055826	4.816067
271.696877	7999.865713	13.630208	-0.055789	4.816067
271.777175	7999.872511	13.635213	-0.055804	4.816068
271.898006	7999.900336	13.640218	-0.055827	4.816076
271.991607	7999.863579	13.645223	-0.055844	4.816064
271.904014	7999.881227	13.650227	-0.055828	4.816070
272.046891	7999.905179	13.655232	-0.055854	4.816076
271.833378	7999.881028	13.660237	-0.055815	4.816070
271.891734	7999.861792	13.665242	-0.055826	4.816064
271.796816	7999.838718	13.670247	-0.055808	4.816058
272.066853	7999.887400	13.675251	-0.055858	4.816071
271.980599	7999.844186	13.680256	-0.055842	4.816059
271.805857	7999.917941	13.685261	-0.055810	4.816081
272.053839	7999.875429	13.690266	-0.055856	4.816068
271.893452	7999.829807	13.695271	-0.055826	4.816055
271.879546	7999.864810	13.700275	-0.055824	4.816065
271.885883	7999.857452	13.705280	-0.055825	4.816063
271.954624	7999.865109	13.710285	-0.055838	4.816065
271.912444	7999.894260	13.715290	-0.055830	4.816074
271.938406	7999.841325	13.720295	-0.055835	4.816058
271.971654	7999.877181	13.725299	-0.055841	4.816069
272.068691	7999.846895	13.730304	-0.055859	4.816059
271.815501	7999.893595	13.735309	-0.055812	4.816074
271.965669	7999.893110	13.740314	-0.055840	4.816073
272.137576	7999.886610	13.745319	-0.055872	4.816070
272.169521	7999.882919	13.750323	-0.055878	4.816069
272.078653	7999.840690	13.755328	-0.055861	4.816057
271.984821	7999.821907	13.760333	-0.055844	4.816052
271.919465	7999.870935	13.765338	-0.055832	4.816067
272.085299	7999.915598	13.770343	-0.055863	4.816079
272.117252	7999.842475	13.775347	-0.055869	4.816058
272.074155	7999.826746	13.780352	-0.055861	4.816053
271.839299	7999.829982	13.785357	-0.055817	4.816055
272.039169	7999.843214	13.790362	-0.055854	4.816058
272.013714	7999.839554	13.795367	-0.055850	4.816057
272.059469	7999.850000	13.800371	-0.055858	4.816060
272.219240	7999.845416	13.805376	-0.055888	4.816058
272.142323	7999.858985	13.810381	-0.055874	4.816062
272.192446	7999.938942	13.815386	-0.055883	4.816085
272.139043	7999.851458	13.820391	-0.055873	4.816060
272.135844	7999.873837	13.825395	-0.055873	4.816067
272.004592	7999.865059	13.830400	-0.055848	4.816065
271.909398	7999.861206	13.835405	-0.055831	4.816064
272.076006	7999.871701	13.840410	-0.055862	4.816066
272.026749	7999.834497	13.845415	-0.055853	4.816056
271.995071	7999.879861	13.850419	-0.055847	4.816069
272.021478	7999.864320	13.855424	-0.055852	4.816064
272.191858	7999.852451	13.860429	-0.055883	4.816060
272.018691	7999.857870	13.865434	-0.055851	4.816063
272.026671	7999.852678	13.870439	-0.055853	4.816061
272.137831	7999.844011	13.875443	-0.055874	4.816058
271.854119	7999.943569	13.880448	-0.055821	4.816089
272.081001	7999.866493	13.885453	-0.055863	4.816065
271.924701	7999.858331	13.890458	-0.055834	4.816063
272.024302	7999.821682	13.895463	-0.055853	4.816052
272.020818	7999.835510	13.900467	-0.055852	4.816056
271.827671	7999.830955	13.905472	-0.055816	4.816056
272.027691	7999.891190	13.910477	-0.055853	4.816072
272.187069	7999.826781	13.915482	-0.055883	4.816053
272.048182	7999.813593	13.920487	-0.055857	4.816049
271.983683	7999.842340	13.925491	-0.055845	4.816058
272.089297	7999.838914	13.930496	-0.055865	4.816057
271.833009	7999.850308	13.935501	-0.055817	4.816061
272.078499	7999.853683	13.940506	-0.055863	4.816061
272.226466	7999.912977	13.945511	-0.055891	4.816078
272.252188	7999.846151	13.950515	-0.055896	4.816058
272.188066	7999.834314	13.955520	-0.055884	4.816055
272.026625	7999.835673	13.960525	-0.055854	4.816056
272.240454	7999.872658	13.965530	-0.055894	4.816066
272.280378	7999.827452	13.970535	-0.055901	4.816052
272.157274	7999.856209	13.975539	-0.055878	4.816061
272.325143	7999.925477	13.980544	-0.055909	4.816081
272.282379	7999.852071	13.985549	-0.055902	4.816059
272.278757	7999.868033	13.990554	-0.055901	4.816064
272.142427	7999.858096	13.995559	-0.055876	4.816062
271.896587	7999.885701	14.000563	-0.055830	4.816071
271.967719	7999.876310	14.005568	-0.055843	4.816068
272.000507	7999.841658	14.010573	-0.055849	4.816058
272.050079	7999.876741	14.015578	-0.055859	4.816068
271.982272	7999.832792	14.020583	-0.055846	4.816055
271.863355	7999.862692	14.025587	-0.055824	4.816065
272.014611	7999.850477	14.030592	-0.055852	4.816060
271.883887	7999.848119	14.035597	-0.055828	4.816060
271.914725	7999.876454	14.040602	-0.055834	4.816069
271.697922	7999.863993	14.045607	-0.055793	4.816066
271.959594	7999.854843	14.050611	-0.055842	4.816062
271.831564	7999.988192	14.055616	-0.055818	4.816102
271.943653	7999.856700	14.060621	-0.055839	4.816063
272.167167	7999.888520	14.065626	-0.055881	4.816071
272.117417	7999.842761	14.070631	-0.055872	4.816058
272.198766	7999.863464	14.075635	-0.055887	4.816063
272.035599	7999.871200	14.080640	-0.055857	4.816066
271.841512	7999.887991	14.085645	-0.055820	4.816072
271.784139	7999.909391	14.090650	-0.055810	4.816079
271.889240	7999.872841	14.095655	-0.055829	4.816068
272.050287	7999.870417	14.100659	-0.055859	4.816066
271.702527	7999.870543	14.105664	-0.055795	4.816068
271.939581	7999.843857	14.110669	-0.055839	4.816059
271.981665	7999.855304	14.115674	-0.055847	4.816062
271.940717	7999.914387	14.120679	-0.055839	4.816079
271.763370	7999.871662	14.125683	-0.055806	4.816068
271.905611	7999.897739	14.130688	-0.055833	4.816075
271.977275	7999.893698	14.135693	-0.055846	4.816073
272.096867	7999.886252	14.140698	-0.055869	4.816070
271.975330	7999.871241	14.145703	-0.055846	4.816067
272.245688	7999.872930	14.150707	-0.055896	4.816066
272.007094	7999.896393	14.155712	-0.055852	4.816074
271.953877	7999.852708	14.160717	-0.055842	4.816061
271.929167	7999.890721	14.165722	-0.055838	4.816073
271.939273	7999.884499	14.170727	-0.055839	4.816071
271.901812	7999.905191	14.175731	-0.055833	4.816077
271.761114	7999.922947	14.180736	-0.055806	4.816083
271.762047	7999.910150	14.185741	-0.055807	4.816079
271.642527	7999.932563	14.190746	-0.055784	4.816086
271.570891	7999.889613	14.195751	-0.055771	4.816074
271.216246	8000.008183	14.200755	-0.055705	4.816111
271.161578	8000.034972	14.205760	-0.055695	4.816119
271.253214	7999.953316	14.210765	-0.055712	4.816094
271.784536	7999.894563	14.215770	-0.055811	4.816074
271.818233	7999.862063	14.220775	-0.055817	4.816065
271.821448	7999.893104	14.225779	-0.055818	4.816074
271.930001	7999.881185	14.230784	-0.055838	4.816070
271.904838	7999.883939	14.235789	-0.055834	4.816071
271.812780	7999.897234	14.240794	-0.055817	4.816075
271.743415	7999.886371	14.245799	-0.055804	4.816072
271.962760	7999.672433	14.250803	-0.055845	4.816009

271.824994	7996.449735	14.255808	-0.055817	4.815067
271.889365	7990.782073	14.260813	-0.055825	4.813410
272.147746	7983.996034	14.265818	-0.055869	4.811424
272.027846	7976.649274	14.270823	-0.055842	4.809274
271.726419	7969.062810	14.275827	-0.055781	4.807055
271.686177	7961.247866	14.280832	-0.055768	4.804766
271.723829	7953.370884	14.285837	-0.055770	4.802458
271.529802	7945.428860	14.290842	-0.055729	4.800130
271.543640	7937.469737	14.295847	-0.055726	4.797796
271.624496	7929.397529	14.300851	-0.055736	4.795426
271.667785	7921.429673	14.305856	-0.055739	4.793087
271.502554	7913.366740	14.310861	-0.055703	4.790719
271.536742	7905.469252	14.315866	-0.055704	4.788398
271.436904	7897.420644	14.320871	-0.055681	4.786032
271.069497	7889.440911	14.325875	-0.055607	4.783686
271.199487	7881.410230	14.330880	-0.055626	4.781322
271.202653	7873.438814	14.335885	-0.055622	4.778974
271.362191	7865.401597	14.340890	-0.055646	4.776605
271.184023	7857.404679	14.345895	-0.055608	4.774249
270.770318	7849.404161	14.350899	-0.055526	4.771891
270.878778	7841.379218	14.355904	-0.055541	4.769523
270.986815	7833.378310	14.360909	-0.055555	4.767160
271.138408	7825.342838	14.365914	-0.055579	4.764787
270.863159	7817.455491	14.370919	-0.055522	4.762457
270.763586	7809.368613	14.375923	-0.055498	4.760066
270.963664	7801.462858	14.380928	-0.055531	4.757727
270.630078	7793.401041	14.385933	-0.055463	4.755342
270.747446	7785.323896	14.390938	-0.055480	4.752950
270.517704	7777.293804	14.395943	-0.055432	4.750572
269.806321	7769.409262	14.400947	-0.055294	4.748238
269.916900	7761.385281	14.405952	-0.055310	4.745858
270.261902	7753.316570	14.410957	-0.055369	4.743463
270.318965	7745.343026	14.415962	-0.055374	4.741096
270.337341	7737.322555	14.420967	-0.055373	4.738714
269.799982	7729.343861	14.425971	-0.055267	4.736345
269.849239	7721.362339	14.430976	-0.055271	4.733972
269.619466	7713.311412	14.435981	-0.055223	4.731578
269.818494	7705.309179	14.440986	-0.055255	4.729196
270.046237	7697.291298	14.445991	-0.055293	4.726808
270.025881	7689.273740	14.450995	-0.055284	4.724419
270.218708	7681.358793	14.456000	-0.055314	4.722060
270.304307	7673.241500	14.461005	-0.055325	4.719639
270.244675	7665.322540	14.466010	-0.055309	4.717277
270.073847	7657.309255	14.471015	-0.055272	4.714885
269.859044	7649.329998	14.476019	-0.055227	4.712503
269.817283	7641.305298	14.481024	-0.055214	4.710105
269.691743	7633.294384	14.486029	-0.055185	4.707710
269.842041	7625.284850	14.491034	-0.055208	4.705314
269.824992	7617.340462	14.496039	-0.055200	4.702937
269.782647	7609.302943	14.501043	-0.055187	4.700530
269.859961	7601.382048	14.506048	-0.055196	4.698157
269.295861	7593.303700	14.511053	-0.055086	4.695737
269.391895	7585.296403	14.516058	-0.055098	4.693336
269.463364	7577.226406	14.521063	-0.055106	4.690915
269.223492	7569.291291	14.526067	-0.055057	4.688533
269.371431	7561.319519	14.531072	-0.055079	4.686139
269.283630	7553.282567	14.536077	-0.055058	4.683724
269.269770	7545.325066	14.541082	-0.055050	4.681331
269.272143	7537.303273	14.546087	-0.055045	4.678918
269.209722	7529.290385	14.551091	-0.055028	4.676507
269.182335	7521.305727	14.556096	-0.055018	4.674103
268.886889	7513.193000	14.561101	-0.054958	4.671659
269.100122	7505.196415	14.566106	-0.054992	4.669248
268.956423	7497.239073	14.571111	-0.054960	4.666849
269.155646	7489.151270	14.576115	-0.054992	4.664408
269.274652	7481.234683	14.581120	-0.055009	4.662018
269.068455	7473.236721	14.586125	-0.054966	4.659602
269.209993	7465.267463	14.591130	-0.054987	4.657194
268.772070	7457.262322	14.596135	-0.054900	4.654774
268.663827	7449.242416	14.601139	-0.054875	4.652348
269.047036	7441.208302	14.606144	-0.054941	4.649915
268.884052	7433.206853	14.611149	-0.054906	4.647492
268.937363	7425.212584	14.616154	-0.054910	4.645070
268.920047	7417.269560	14.621159	-0.054902	4.642662
268.781284	7409.264372	14.626163	-0.054871	4.640234
268.664987	7401.292310	14.631168	-0.054844	4.637815
268.753007	7393.171969	14.636173	-0.054855	4.635349
268.765319	7385.199523	14.641178	-0.054853	4.632927
268.667616	7377.184726	14.646183	-0.054829	4.630491
268.368082	7369.192126	14.651187	-0.054768	4.628060
268.372699	7361.225119	14.656192	-0.054764	4.625636
268.024877	7353.233809	14.661197	-0.054694	4.623203
268.025205	7345.219912	14.666202	-0.054689	4.620762
268.240616	7337.207593	14.671207	-0.054724	4.618320
268.187056	7329.192838	14.676211	-0.054709	4.615876
267.894022	7321.221894	14.681216	-0.054649	4.613445
267.960697	7313.137140	14.686221	-0.054656	4.610977
268.126090	7305.178416	14.691226	-0.054682	4.608546
268.153293	7297.158339	14.696231	-0.054682	4.606095
268.066928	7289.175113	14.701235	-0.054661	4.603654
268.275466	7281.195299	14.706240	-0.054694	4.601213
268.031222	7273.214396	14.711245	-0.054644	4.598771
268.073569	7265.223609	14.716250	-0.054646	4.596324
267.977081	7257.175955	14.721255	-0.054623	4.593858
267.803422	7249.080765	14.726259	-0.054586	4.591376
267.837799	7241.129341	14.731264	-0.054587	4.588937
267.827838	7233.105892	14.736269	-0.054580	4.586475
267.803803	7225.136582	14.741274	-0.054570	4.584028
267.544038	7217.173821	14.746279	-0.054517	4.581581
267.326951	7209.158509	14.751283	-0.054471	4.579118
267.206260	7201.236773	14.756288	-0.054443	4.576681
267.424980	7193.109817	14.761293	-0.054479	4.574180
267.391381	7185.118457	14.766298	-0.054468	4.571720
267.477388	7177.086601	14.771303	-0.054478	4.569246
267.496735	7169.117950	14.776307	-0.054477	4.566790
267.318472	7161.147988	14.781312	-0.054439	4.564332
267.189174	7153.163051	14.786317	-0.054409	4.561868
267.302330	7145.136315	14.791322	-0.054425	4.559390
267.121406	7137.200673	14.796327	-0.054386	4.556939
267.228568	7129.097792	14.801331	-0.054401	4.554434
267.195404	7121.139096	14.806336	-0.054390	4.551973
267.013418	7113.065212	14.811341	-0.054351	4.549475
266.978687	7105.120308	14.816346	-0.054339	4.547016
266.986953	7097.098939	14.821351	-0.054335	4.544531
267.017571	7089.121147	14.826355	-0.054336	4.542059
266.873206	7081.159530	14.831360	-0.054304	4.539590
266.420228	7073.226851	14.836365	-0.054214	4.537128
266.715681	7065.145296	14.841370	-0.054264	4.534620
266.547875	7057.099537	14.846375	-0.054228	4.532121
266.393144	7049.075297	14.851379	-0.054194	4.529627
266.499249	7041.117394	14.856384	-0.054208	4.527153
266.565660	7033.077747	14.861389	-0.054216	4.524652
266.415089	7025.160083	14.866394	-0.054183	4.522187
266.590293	7017.145663	14.871399	-0.054210	4.519691
266.666181	7009.190302	14.876403	-0.054219	4.517212
266.544167	7001.130419	14.881408	-0.054191	4.514699
266.352066	6992.982492	14.886413	-0.054150	4.512157
266.290986	6985.080344	14.891418	-0.054134	4.509690
266.141797	6977.082223	14.896423	-0.054101	4.507192
266.146320	6969.022591	14.901427	-0.054096	4.504673
266.238799	6961.162489	14.906432	-0.054108	4.502216
266.093081	6953.041048	14.911437	-0.054076	4.499675
266.052693	6945.117893	14.916442	-0.054063	4.497195
265.922165	6937.050355	14.921447	-0.054034	4.494668
265.961012	6929.041824	14.926451	-0.054036	4.492159
265.812646	6921.078132	14.931456	-0.054003	4.489661
265.916089	6913.072036	14.936461	-0.054017	4.487150
265.915303	6905.054388	14.941466	-0.054012	4.484633
265.942977	6897.124476	14.946471	-0.054012	4.482143
265.709690	6889.074194	14.951475	-0.053963	4.479612
265.550047	6881.121192	14.956480	-0.053928	4.477111
265.628769	6873.022633	14.961485	-0.053938	4.474564
265.688982	6865.039894	14.966490	-0.053944	4.472051
265.481744	6857.032542	14.971495	-0.053900	4.469529
265.561977	6849.025930	14.976499	-0.053910	4.467006
265.602696	6841.044018	14.981504	-0.053912	4.464489
265.292543	6833.091027	14.986509	-0.053850	4.461979
265.359866	6825.045698	14.991514	-0.053857	4.459440
265.432324	6817.089860	14.996519	-0.053865	4.456927
265.346501	6809.026653	15.001523	-0.053844	4.454379
265.325448	6801.028575	15.006528	-0.053835	4.451849
265.139120	6793.020171	15.011533	-0.053795	4.449315
265.013338	6785.033457	15.016538	-0.053766	4.446786
265.089341	6777.038129	15.021543	-0.053775	4.444254
265.054106	6769.034881	15.026547	-0.053764	4.441717
265.203331	6761.062524	15.031552	-0.053786	4.439190
265.010137	6753.054626	15.036557	-0.053745	4.436648
265.037009	6745.009314	15.041562	-0.053745	4.434094
264.911497	6736.998090	15.046567	-0.053717	4.431549
264.930220	6728.945470	15.051571	-0.053715	4.428989
264.827709	6720.979574	15.056576	-0.053691	4.426455
264.801559	6712.978036	15.061581	-0.053681	4.423909
264.889015	6705.018796	15.066586	-0.053692	4.421375
264.821719	6697.028988	15.071591	-0.053674	4.418830
264.606589	6689.000839	15.076595	-0.053629	4.416270
264.678921	6681.021328	15.081600	-0.053637	4.413725
264.455672	6672.962612	15.086605	-0.053590	4.411152
264.537301	6664.991260	15.091610	-0.053600	4.408607
264.382451	6657.038710	15.096615	-0.053566	4.406065
264.260986	6649.023934	15.101619	-0.053539	4.403502
264.407734	6641.010806	15.106624	-0.053561	4.400940
264.334849	6632.986152	15.111629	-0.053542	4.398371
264.453501	6624.983721	15.116634	-0.053559	4.395809
264.087221	6616.996446	15.121639	-0.053486	4.393248
264.260263	6608.955773	15.126643	-0.053513	4.390670
264.021411	6601.058690	15.131648	-0.053463	4.388136
263.819948	6592.973153	15.136653	-0.053420	4.385539
263.949168	6584.990048	15.141658	-0.053439	4.382976
264.084440	6576.992047	15.146663	-0.053459	4.380406
263.945828	6569.041162	15.151667	-0.053428	4.377848
263.805553	6561.048455	15.156672	-0.053397	4.375276
263.697746	6552.986277	15.161677	-0.053372	4.372680
263.548732	6545.020729	15.166682	-0.053339	4.370113
263.519467	6537.025863	15.171687	-0.053328	4.367535
263.472467	6528.941220	15.176691	-0.053314	4.364928
263.734263	6521.044454	15.181696	-0.053358	4.362381
263.443394	6513.016326	15.186701	-0.053299	4.359787
263.522491	6505.050040	15.191706	-0.053308	4.357213
263.338796	6496.985205	15.196711	-0.053269	4.354605
263.123281	6488.865101	15.201715	-0.053223	4.351977
263.354718	6480.907347	15.206720	-0.053261	4.349402
263.120896	6472.965081	15.211725	-0.053213	4.346828
263.128850	6464.972851	15.216730	-0.053209	4.344238
263.197437	6456.992866	15.221735	-0.053217	4.341651
262.945119	6448.975873	15.226739	-0.053164	4.339048
263.124589	6440.984972	15.231744	-0.053193	4.336455
263.052681	6432.973115	15.236749	-0.053174	4.333852
262.934132	6424.970900	15.241754	-0.053147	4.331250
263.085847	6417.020768	15.246759	-0.053170	4.328666
262.871402	6408.939080	15.251763	-0.053125	4.326034
262.855633	6401.010632	15.256768	-0.053117	4.323452
262.951245	6392.929403	15.261773	-0.053129	4.320820
262.849809	6384.940560	15.266778	-0.053105	4.318214
263.005802	6376.973045	15.271783	-0.053129	4.315616
262.710551	6368.924470	15.276787	-0.053069	4.312987
262.822479	6360.949398	15.281792	-0.053085	4.310383
262.624502	6352.975461	15.286797	-0.053043	4.307775
262.741981	6344.903959	15.291802	-0.053059	4.305137
262.590808	6336.978856	15.296807	-0.053026	4.302542
262.373980	6328.941895	15.301811	-0.052981	4.299909
262.370741	6320.996510	15.306816	-0.052975	4.297306
262.448136	6312.947457	15.311821	-0.052984	4.294668
262.569678	6304.912762	15.316826	-0.053002	4.292033
262.403037	6296.938227	15.321831	-0.052965	4.289414
262.024988	6288.952740	15.326835	-0.052890	4.286789
262.516216	6280.932545	15.331840	-0.052976	4.284157
262.196315	6272.987876	15.336845	-0.052911	4.281542
262.047587	6264.917886	15.341850	-0.052879	4.278885
261.919301	6256.988032	15.346855	-0.052850	4.276274
261.965730	6248.901510	15.351859	-0.052853	4.273610
261.972591	6240.914733	15.356864	-0.052849	4.270977
261.941083	6232.887485	15.361869	-0.052838	4.268329
261.979714	6224.888052	15.366874	-0.052840	4.265689
261.941309	6216.959786	15.371879	-0.052828	4.263070
261.730312	6208.881233	15.376883	-0.052783	4.260399
261.725960	6200.954457	15.381888	-0.052777	4.257778
261.681528	6192.861945	15.386893	-0.052764	4.255100
261.693311	6184.905992	15.391898	-0.052761	4.252466
261.632019	6176.870233	15.396903	-0.052744	4.249803
261.548808	6168.958752	15.401907	-0.052724	4.247179
261.476617	6160.915477	15.406912	-0.052705	4.244511
261.360982	6152.979082	15.411917	-0.052678	4.241875
261.346633	6144.914300	15.416922	-0.052671	4.239197
261.264143	6136.999240	15.421927	-0.052650	4.236565
261.086446	6128.920017	15.426931	-0.052612	4.233877
261.483793	6120.955704	15.431936	-0.052681	4.231231
261.449913	6112.902371	15.436941	-0.052669	4.228549
261.360822	6104.919423	15.441946	-0.052647	4.225888
261.321797	6096.951359	15.446951	-0.052635	4.223231
261.148733	6088.925739	15.451955	-0.052598	4.220552
261.201720	6080.979196	15.456960	-0.052602	4.217900
261.084945	6072.941642	15.461965	-0.052575	4.215214
261.156993	6064.938310	15.466970	-0.052584	4.212540
261.054829	6056.925556	15.471975	-0.052559	4.209859
260.749161	6048.964070	15.476979	-0.052497	4.207192
261.042727	6040.949866	15.481984	-0.052547	4.204511
260.802008	6033.002296	15.486989	-0.052497	4.201845
260.648784	6024.989290	15.491994	-0.052463	4.199157
260.582422	6016.979782	15.496999	-0.052446	4.196469
260.625832	6008.880061	15.502003	-0.052449	4.193750
260.696386	6000.839558	15.507008	-0.052456	4.191049
260.459676	5992.876848	15.512013	-0.052407	4.188370
260.495173	5984.859839	15.517018	-0.052409	4.185674
260.547391	5976.953166	15.522023	-0.052413	4.183013
260.268246	5968.928519	15.527027	-0.052356	4.180307
260.457917	5960.949889	15.532032	-0.052386	4.177620
260.323294	5952.921887	15.537037	-0.052356	4.174911
260.173745	5944.921833	15.542042	-0.052323	4.172209
260.049458	5936.904957	15.547047	-0.052295	4.169501
260.015969	5928.949510	15.552051	-0.052283	4.166812
260.244357	5920.912208	15.557056	-0.052321	4.164097
259.986710	5912.943080	15.562061	-0.052268	4.161398
259.903246	5904.931997	15.567066	-0.052247	4.158684
259.884242	5896.939700	15.572071	-0.052238	4.155976
259.638535	5888.890249	15.577075	-0.052187	4.153245
259.817574	5880.895386	15.582080	-0.052215	4.150534
259.900480	5872.888707	15.587085	-0.052226	4.147817
259.778312	5864.902498	15.592090	-0.052198	4.145103
259.630028	5856.960117	15.597095	-0.052165	4.142402
259.653422	5848.883110	15.602099	-0.052164	4.139654
259.722265	5840.934594	15.607104	-0.052172	4.136950
259.691393	5832.942496	15.612109	-0.052161	4.134227
259.623024	5824.900219	15.617114	-0.052143	4.131486
259.500111	5816.917401	15.622119	-0.052115	4.128762
259.447123	5808.888963	15.627123	-0.052100	4.126021
259.440588	5800.934605	15.632128	-0.052094	4.123305
259.434791	5792.941635	15.637133	-0.052087	4.120573
259.327549	5784.957625	15.642138	-0.052062	4.117842
259.272407	5776.946069	15.647143	-0.052047	4.115100
259.137031	5768.886291	15.652147	-0.052016	4.112339
259.150229	5760.900335	15.657152	-0.052014	4.109602
258.947875	5752.912152	15.662157	-0.051971	4.106861
258.959868	5744.881446	15.667162	-0.051968	4.104106
258.948393	5736.946092	15.672167	-0.051961	4.101381
258.870432	5728.912221	15.677171	-0.051941	4.098620
259.028957	5720.954810	15.682176	-0.051965	4.095886
258.840046	5712.913255	15.687181	-0.051925	4.093118
259.011558	5704.890749	15.692186	-0.051952	4.090358
258.785403	5696.951272	15.697191	-0.051904	4.087620
258.718040	5688.920593	15.702195	-0.051887	4.084851
258.712510	5680.986201	15.707200	-0.051881	4.082114
258.765291	5672.993400	15.712205	-0.051885	4.079355
258.502276	5664.993887	15.717210	-0.051831	4.076589
258.630836	5656.944877	15.722215	-0.051850	4.073808
258.620589	5648.905870	15.727219	-0.051843	4.071028
258.471176	5640.941885	15.732224	-0.051810	4.068269
258.404987	5632.950331	15.737229	-0.051792	4.065500
258.258671	5624.984563	15.742234	-0.051760	4.062737
258.169425	5616.978802	15.747239	-0.051738	4.059959
258.233382	5608.996671	15.752243	-0.051745	4.057190
258.414148	5600.964921	15.757248	-0.051773	4.054403
258.054981	5592.936345	15.762253	-0.051701	4.051607
257.944474	5584.919456	15.767258	-0.051676	4.048817
258.056585	5576.967154	15.772263	-0.051691	4.046051
257.966441	5568.985583	15.777267	-0.051669	4.043270
258.048682	5560.959418	15.782272	-0.051679	4.040474
257.929248	5553.008034	15.787277	-0.051652	4.037699
257.949155	5544.961551	15.792282	-0.051651	4.034891
257.660576	5536.885385	15.797287	-0.051592	4.032066
257.451465	5528.874160	15.802291	-0.051548	4.029264
257.583509	5520.922837	15.807296	-0.051567	4.026485
257.528879	5512.914466	15.812301	-0.051552	4.023681
257.418753	5504.931015	15.817306	-0.051526	4.020883
257.448606	5496.962290	15.822311	-0.051526	4.018091
257.311815	5488.932441	15.827315	-0.051496	4.015273
257.486348	5480.922346	15.832320	-0.051523	4.012464
257.437230	5472.881337	15.837325	-0.051509	4.009640
257.163385	5464.966867	15.842330	-0.051453	4.006854
257.240987	5456.963583	15.847335	-0.051462	4.004040
257.090980	5448.982165	15.852339	-0.051429	4.001229
257.145344	5440.978746	15.857344	-0.051434	3.998411
257.040046	5432.978331	15.862349	-0.051409	3.995590
256.921917	5424.901016	15.867354	-0.051382	3.992739
257.037260	5416.908334	15.872359	-0.051398	3.989920
257.078526	5408.912235	15.877363	-0.051401	3.987096
257.084292	5400.931347	15.882368	-0.051397	3.984276
257.036251	5392.956803	15.887373	-0.051383	3.981454
257.037148	5384.945140	15.892378	-0.051378	3.978618
256.988093	5376.975853	15.897383	-0.051363	3.975795
256.806897	5368.938231	15.902387	-0.051324	3.972943
256.773027	5360.926911	15.907392	-0.051313	3.970101
256.583262	5352.979599	15.912397	-0.051272	3.967277
256.654759	5344.946752	15.917402	-0.051281	3.964424
256.492544	5337.017547	15.922407	-0.051245	3.961603
256.460531	5329.022132	15.927411	-0.051234	3.958758
256.472019	5321.038316	15.932416	-0.051231	3.955916
256.326057	5312.971356	15.937421	-0.051199	3.953040
256.421250	5304.934723	15.942426	-0.051211	3.950176
256.445890	5296.965873	15.947431	-0.051211	3.947334
256.323919	5288.975721	15.952435	-0.051183	3.944479
256.412102	5281.025811	15.957440	-0.051194	3.941640
256.341634	5273.014224	15.962445	-0.051176	3.938774
256.291218	5264.999678	15.967450	-0.051161	3.935906
256.179024	5257.030630	15.972455	-0.051135	3.933051
256.216949	5248.986025	15.977459	-0.051137	3.930169
256.245927	5241.042618	15.982464	-0.051137	3.927321
256.021860	5233.007902	15.987469	-0.051090	3.924434
255.906241	5225.052031	15.992474	-0.051064	3.921574
255.872862	5217.027578	15.997479	-0.051052	3.918690
255.743310	5209.032958	16.002483	-0.051023	3.915812
255.756474	5201.026700	16.007488	-0.051020	3.912931
256.004333	5192.950384	16.012493	-0.051061	3.910027
255.853303	5185.006665	16.017498	-0.051028	3.907161
255.721372	5177.002985	16.022503	-0.050998	3.904271
255.659468	5169.014689	16.027507	-0.050982	3.901387
255.692721	5161.032644	16.032512	-0.050983	3.898504
255.645770	5153.045944	16.037517	-0.050969	3.895616
255.574214	5145.000904	16.042522	-0.050950	3.892704
255.561442	5137.009732	16.047527	-0.050943	3.889810
255.260978	5129.050677	16.052531	-0.050882	3.886921
255.484007	5121.032481	16.057536	-0.050918	3.884018
255.437641	5113.028284	16.062541	-0.050904	3.881112
255.106739	5105.060540	16.067546	-0.050837	3.878213
255.235284	5097.060913	16.072551	-0.050856	3.875308
254.990989	5088.817546	16.077555	-0.050805	3.872305
254.908486	5080.868753	16.082560	-0.050785	3.869410
254.824801	5072.913162	16.087565	-0.050764	3.866511
254.808584	5064.955686	16.092570	-0.050756	3.863610
254.917208	5056.988933	16.097575	-0.050771	3.860706
254.954095	5049.001231	16.102579	-0.050773	3.857791
254.899777	5041.023642	16.107584	-0.050758	3.854875
254.679443	5033.000538	16.112589	-0.050711	3.851937
254.597199	5025.037535	16.117594	-0.050691	3.849022
254.679955	5017.051121	16.122599	-0.050701	3.846099
254.611177	5009.043306	16.127603	-0.050683	3.843163
254.402249	5001.091919	16.132608	-0.050639	3.840243
254.419842	4993.107787	16.137613	-0.050637	3.837313
254.438855	4985.062552	16.142618	-0.050636	3.834358
254.361879	4977.068766	16.147623	-0.050616	3.831418
254.171060	4969.048496	16.152627	-0.050575	3.828464
254.317659	4961.055419	16.157632	-0.050598	3.825524
254.149729	4953.075124	16.162637	-0.050561	3.822580
253.909866	4945.084806	16.167642	-0.050511	3.819629
253.979523	4937.150886	16.172647	-0.050519	3.816703
254.055247	4929.062966	16.177651	-0.050528	3.813718
253.922064	4921.065049	16.182656	-0.050498	3.810759
254.011914	4913.118009	16.187661	-0.050510	3.807821
254.025823	4905.078576	16.192666	-0.050507	3.804846
254.135943	4897.148560	16.197671	-0.050522	3.801911
253.734237	4889.133020	16.202675	-0.050442	3.798930
253.898359	4881.148303	16.207680	-0.050468	3.795971
253.973181	4873.108551	16.212685	-0.050477	3.792988
253.662813	4865.074936	16.217690	-0.050414	3.789995
253.592618	4857.120155	16.222695	-0.050395	3.787035
253.401603	4849.110822	16.227699	-0.050355	3.784050
253.495010	4841.120434	16.232704	-0.050367	3.781076
253.410867	4833.168579	16.237709	-0.050346	3.778110
253.157803	4825.102559	16.242714	-0.050294	3.775095
253.364414	4817.126860	16.247719	-0.050327	3.772121
253.112823	4809.067014	16.252723	-0.050275	3.769104
253.163482	4801.104085	16.257728	-0.050279	3.766127
253.201391	4793.124022	16.262733	-0.050281	3.763141
253.009794	4785.116655	16.267738	-0.050240	3.760138
253.010073	4777.199053	16.272743	-0.050235	3.757169
253.001997	4769.131008	16.277747	-0.050229	3.754142
253.061010	4761.109440	16.282752	-0.050234	3.751132
253.110561	4753.104007	16.287757	-0.050239	3.748125
253.042227	4745.096450	16.292762	-0.050221	3.745112
252.861942	4737.202593	16.297767	-0.050182	3.742136
252.661742	4729.175487	16.302771	-0.050140	3.739108
252.734845	4721.207582	16.307776	-0.050148	3.736106
252.710783	4713.193367	16.312781	-0.050138	3.733082
252.617676	4705.123026	16.317786	-0.050116	3.730032
252.542816	4697.206006	16.322791	-0.050097	3.727038
252.460739	4689.187748	16.327795	-0.050076	3.724004
252.532379	4681.188655	16.332800	-0.050084	3.720978
252.394615	4673.234799	16.337805	-0.050054	3.717961
252.203012	4665.229142	16.342810	-0.050013	3.714921
252.298611	4657.136225	16.347815	-0.050025	3.711853
252.102639	4649.121132	16.352819	-0.049984	3.708804
252.117887	4641.155876	16.357824	-0.049981	3.705777
252.086367	4633.199306	16.362829	-0.049970	3.702750
252.143209	4625.161611	16.367834	-0.049976	3.699691
251.974102	4617.270427	16.372839	-0.049939	3.696680
252.014336	4609.224907	16.377843	-0.049942	3.693613
252.067832	4601.199915	16.382848	-0.049946	3.690552
251.907168	4593.246971	16.387853	-0.049911	3.687510
251.675130	4585.236755	16.392858	-0.049863	3.684442
251.769318	4577.300053	16.397863	-0.049875	3.681408
251.671182	4569.274096	16.402867	-0.049852	3.678332
251.565856	4561.266775	16.407872	-0.049827	3.675260
251.469834	4553.265586	16.412877	-0.049804	3.672189
251.618466	4545.230546	16.417882	-0.049827	3.669108
251.538648	4537.262857	16.422887	-0.049806	3.666045
251.504346	4529.270432	16.427891	-0.049795	3.662971
251.531473	4521.234414	16.432896	-0.049795	3.659878
251.619855	4513.302348	16.437901	-0.049806	3.656825
251.252504	4505.291748	16.442906	-0.049733	3.653728
251.568734	4497.262248	16.447911	-0.049786	3.650638
251.439016	4489.284916	16.452915	-0.049757	3.647554
251.377347	4481.266986	16.457920	-0.049740	3.644454
251.221723	4473.326035	16.462925	-0.049706	3.641378
251.139452	4465.318351	16.467930	-0.049686	3.638275
251.109483	4457.352621	16.472935	-0.049675	3.635188
250.977972	4449.288790	16.477939	-0.049645	3.632057
250.956338	4441.291955	16.482944	-0.049636	3.628953
250.831352	4433.302681	16.487949	-0.049608	3.625846
250.591768	4425.300152	16.492954	-0.049558	3.622728
250.665664	4417.330195	16.497959	-0.049567	3.619628
250.760694	4409.355151	16.502963	-0.049579	3.616525
250.726535	4401.336688	16.507968	-0.049568	3.613398
250.699568	4393.336681	16.512973	-0.049557	3.610276
250.730027	4385.344378	16.517978	-0.049558	3.607156
250.701584	4377.376700	16.522983	-0.049547	3.604041
250.502692	4369.380085	16.527987	-0.049505	3.600908
250.478261	4361.433982	16.532992	-0.049496	3.597796
250.378089	4353.413337	16.537997	-0.049472	3.594650
250.419974	4345.382500	16.543002	-0.049474	3.591502
250.407642	4337.407872	16.548007	-0.049467	3.588371
250.333052	4329.376359	16.553011	-0.049448	3.585213
250.282047	4321.432802	16.558016	-0.049433	3.582088
250.199978	4313.457210	16.563021	-0.049413	3.578947
250.169027	4305.435069	16.568026	-0.049402	3.575786
250.014174	4297.453535	16.573031	-0.049368	3.572634
249.944339	4289.403369	16.578035	-0.049350	3.569456
249.993953	4281.432317	16.583040	-0.049354	3.566309
250.040857	4273.464534	16.588045	-0.049357	3.563160
249.693967	4265.461572	16.593050	-0.049288	3.559983
249.768120	4257.515442	16.598055	-0.049296	3.556839
249.658505	4249.430784	16.603059	-0.049271	3.553631
249.577729	4241.340346	16.608064	-0.049250	3.550419
249.502648	4233.411661	16.613069	-0.049231	3.547268
249.594791	4225.400735	16.618074	-0.049243	3.544087
249.495563	4217.477064	16.623079	-0.049220	3.540931
249.298788	4209.504285	16.628083	-0.049178	3.537751
249.404471	4201.464520	16.633088	-0.049192	3.534550
249.360088	4193.485468	16.638093	-0.049179	3.531366
249.106791	4185.463657	16.643098	-0.049127	3.528156
249.191486	4177.469918	16.648103	-0.049137	3.524964
249.135812	4169.535322	16.653107	-0.049122	3.521788
249.060874	4161.528304	16.658112	-0.049103	3.518580
248.925233	4153.566715	16.663117	-0.049072	3.515386
248.784687	4145.531888	16.668122	-0.049041	3.512159
249.138959	4137.516562	16.673127	-0.049102	3.508952
248.789431	4129.518678	16.678131	-0.049031	3.505728
248.698676	4121.569796	16.683136	-0.049009	3.502528
248.881119	4113.545234	16.688141	-0.049038	3.499303
248.714967	4105.543206	16.693146	-0.049002	3.496074
248.690207	4097.586489	16.698151	-0.048992	3.492864
248.865666	4089.551267	16.703155	-0.049020	3.489626
248.927265	4081.591727	16.708160	-0.049026	3.486412
248.613958	4073.626986	16.713165	-0.048963	3.483181
248.506710	4065.622117	16.718170	-0.048937	3.479937
248.326169	4057.704429	16.723175	-0.048899	3.476723
248.207124	4049.626981	16.728179	-0.048871	3.473444
248.105000	4041.595097	16.733184	-0.048847	3.470180
248.269918	4033.622759	16.738189	-0.048873	3.466946
248.152431	4025.624065	16.743194	-0.048846	3.463689
248.194668	4017.642547	16.748199	-0.048848	3.460441
248.099534	4009.649535	16.753203	-0.048826	3.457181
248.111761	4001.641804	16.758208	-0.048823	3.453916
247.835525	3993.676867	16.763213	-0.048766	3.450655
247.700710	3985.703710	16.768218	-0.048736	3.447392
247.966052	3977.639746	16.773223	-0.048780	3.444103
247.754788	3969.712334	16.778227	-0.048736	3.440850
247.635632	3961.726474	16.783232	-0.048708	3.437574
247.686764	3953.755851	16.788237	-0.048713	3.434306
247.504278	3945.682486	16.793242	-0.048673	3.430985
247.607246	3937.692594	16.798247	-0.048687	3.427705
247.563575	3929.682019	16.803251	-0.048674	3.424408
247.455090	3921.761003	16.808256	-0.048649	3.421143
247.340418	3913.773915	16.813261	-0.048622	3.417847
247.091990	3905.760913	16.818266	-0.048571	3.414532
247.417048	3897.754100	16.823271	-0.048626	3.411237
247.180241	3889.773906	16.828275	-0.048577	3.407930
247.189289	3881.776029	16.833280	-0.048574	3.404621
247.245446	3873.814433	16.838285	-0.048579	3.401325
247.018894	3865.831256	16.843290	-0.048531	3.398008
247.157386	3857.826436	16.848295	-0.048552	3.394691
247.108873	3849.709723	16.853299	-0.048538	3.391318
247.011459	3841.777047	16.858304	-0.048515	3.388016
246.856593	3833.784234	16.863309	-0.048481	3.384684
246.807778	3825.821191	16.868314	-0.048466	3.381364
246.847541	3817.857808	16.873319	-0.048469	3.378045
246.633575	3809.871272	16.878323	-0.048424	3.374703
246.602589	3801.851923	16.883328	-0.048413	3.371351
246.596542	3793.885458	16.888333	-0.048406	3.368019
246.555806	3785.829960	16.893338	-0.048394	3.364644
246.442321	3777.922762	16.898343	-0.048367	3.361326
246.341632	3769.930110	16.903347	-0.048343	3.357970
246.414515	3761.905424	16.908352	-0.048352	3.354602
246.208001	3753.893367	16.913357	-0.048308	3.351227
246.243181	3745.876920	16.918362	-0.048310	3.347855
246.509823	3737.905686	16.923367	-0.048354	3.344507
246.135803	3729.959011	16.928371	-0.048279	3.341142
245.873222	3721.985027	16.933376	-0.048225	3.337767
246.195043	3713.959812	16.938381	-0.048280	3.334388
246.235737	3705.917528	16.943386	-0.048282	3.330988
246.053142	3697.972866	16.948391	-0.048243	3.327618
245.800593	3690.014458	16.953395	-0.048191	3.324236
245.958760	3681.987227	16.958400	-0.048215	3.320836
245.888511	3674.040301	16.963405	-0.048197	3.317459
245.616467	3666.030382	16.968410	-0.048141	3.314044
245.552033	3658.023807	16.973415	-0.048124	3.310634
245.638054	3650.002741	16.978419	-0.048135	3.307221
245.518280	3642.013940	16.983424	-0.048108	3.303810
245.601970	3634.060042	16.988429	-0.048118	3.300418
245.457571	3626.078279	16.993434	-0.048086	3.297002
245.510138	3618.072041	16.998439	-0.048091	3.293579
245.560889	3610.060419	17.003443	-0.048095	3.290150
245.467245	3602.098406	17.008448	-0.048072	3.286734
245.267645	3594.146926	17.013453	-0.048030	3.283314
244.977966	3586.160327	17.018458	-0.047971	3.279873
245.119231	3578.194339	17.023463	-0.047992	3.276453
245.177390	3570.139697	17.028467	-0.047998	3.272988
244.990379	3562.109163	17.033472	-0.047958	3.269520
245.019660	3554.161725	17.038477	-0.047958	3.266093
245.019504	3546.158805	17.043482	-0.047953	3.262638
245.032449	3538.170397	17.048487	-0.047950	3.259185
244.784612	3530.190387	17.053491	-0.047899	3.255722
244.870864	3522.178439	17.058496	-0.047910	3.252255
244.913502	3514.186899	17.063501	-0.047912	3.248791
244.676755	3506.197107	17.068506	-0.047863	3.245313
244.688084	3498.273647	17.073511	-0.047860	3.241870
244.666234	3490.286344	17.078515	-0.047851	3.238394
244.387807	3482.296174	17.083520	-0.047794	3.234903
244.512335	3474.216715	17.088525	-0.047812	3.231386
244.419183	3466.219048	17.093530	-0.047789	3.227891
244.479266	3458.220876	17.098535	-0.047795	3.224399
244.203068	3450.282576	17.103539	-0.047739	3.220916
244.190333	3442.295683	17.108544	-0.047731	3.217418
244.193210	3434.324570	17.113549	-0.047727	3.213923
244.145908	3426.288608	17.118554	-0.047713	3.210395
244.096107	3418.337738	17.123559	-0.047698	3.206900
244.170437	3410.318633	17.128563	-0.047707	3.203376
244.099163	3402.350371	17.133568	-0.047689	3.199865
243.838088	3394.439942	17.138573	-0.047635	3.196367
243.697969	3386.395348	17.143578	-0.047604	3.192812
243.545815	3378.428735	17.148583	-0.047570	3.189286
243.539084	3370.388066	17.153587	-0.047564	3.185730
243.413270	3362.433248	17.158592	-0.047535	3.182202
243.349695	3354.480681	17.163597	-0.047518	3.178675
243.339540	3346.445384	17.168602	-0.047511	3.175109
243.422695	3338.457254	17.173607	-0.047521	3.171564
243.524027	3330.448211	17.178611	-0.047535	3.168006
243.511591	3322.428211	17.183616	-0.047528	3.164435
243.485230	3314.532018	17.188621	-0.047518	3.160914
243.089959	3306.586524	17.193626	-0.047439	3.157352
243.256553	3298.547001	17.198631	-0.047465	3.153767
243.100281	3290.514319	17.203635	-0.047430	3.150168
242.929780	3282.534788	17.208640	-0.047394	3.146588
243.047008	3274.557330	17.213645	-0.047410	3.143017
243.042155	3266.534032	17.218650	-0.047404	3.139416
243.010902	3258.605858	17.223655	-0.047393	3.135852
242.966980	3250.592227	17.228659	-0.047380	3.132246
242.617304	3242.636527	17.233664	-0.047310	3.128648
242.673512	3234.637838	17.238669	-0.047315	3.125044
242.760479	3226.646014	17.243674	-0.047326	3.121441
242.788005	3218.705834	17.248679	-0.047326	3.117854
242.411844	3210.734659	17.253683	-0.047251	3.114231
242.434180	3202.668065	17.258688	-0.047250	3.110578
242.507345	3194.697406	17.263693	-0.047258	3.106967
242.412780	3186.721723	17.268698	-0.047235	3.103342
242.442289	3178.731386	17.273703	-0.047236	3.099711
242.336086	3170.764623	17.278707	-0.047211	3.096081
242.105859	3162.783362	17.283712	-0.047163	3.092434
242.208016	3154.740723	17.288717	-0.047177	3.088770
242.051685	3146.777243	17.293722	-0.047142	3.085126
242.018152	3138.841615	17.298727	-0.047131	3.081496
242.047819	3130.828562	17.303731	-0.047131	3.077829
242.063801	3122.818257	17.308736	-0.047129	3.074159
242.175081	3114.751439	17.313741	-0.047145	3.070462
242.079577	3106.766848	17.318746	-0.047122	3.066789
242.033802	3098.826168	17.323751	-0.047108	3.063135
242.087472	3090.841513	17.328755	-0.047113	3.059460
242.111549	3082.883653	17.333760	-0.047112	3.055792
241.887233	3074.927581	17.338765	-0.047065	3.052109
241.857741	3066.907969	17.343770	-0.047055	3.048401
241.933082	3058.906941	17.348775	-0.047064	3.044702
241.623266	3051.000271	17.353779	-0.047001	3.041024
241.412361	3043.029925	17.358784	-0.046956	3.037316
241.528592	3035.015547	17.363789	-0.046973	3.033600
241.346053	3026.994823	17.368794	-0.046934	3.029861
241.330918	3019.042496	17.373799	-0.046926	3.026158
241.252503	3011.071001	17.378803	-0.046906	3.022438
241.230416	3003.061398	17.383808	-0.046897	3.018698
241.096574	2995.094727	17.388813	-0.046867	3.014969
241.052782	2987.066583	17.393818	-0.046853	3.011210
241.256950	2979.085192	17.398823	-0.046886	3.007481
241.048040	2971.106268	17.403827	-0.046842	3.003728
240.922816	2963.139946	17.408832	-0.046814	2.999980
240.904445	2955.198963	17.413837	-0.046805	2.996245
240.901894	2947.154240	17.418842	-0.046799	2.992457
240.828049	2939.179505	17.423847	-0.046781	2.988694
240.771349	2931.178673	17.428851	-0.046765	2.984915
240.716368	2923.210929	17.433856	-0.046749	2.981146
240.735620	2915.261903	17.438861	-0.046748	2.977385
240.658788	2907.242248	17.443866	-0.046728	2.973581
240.567316	2899.266020	17.448871	-0.046706	2.969793
240.522516	2891.278626	17.453875	-0.046693	2.965996
240.286999	2883.334311	17.458880	-0.046644	2.962205
240.227830	2875.372910	17.463885	-0.046628	2.958410
240.300150	2867.359251	17.468890	-0.046636	2.954592
240.228016	2859.366848	17.473895	-0.046617	2.950772
239.990334	2851.382411	17.478899	-0.046568	2.946943
240.187627	2843.351836	17.483904	-0.046599	2.943108
240.214050	2835.419708	17.488909	-0.046599	2.939307
240.068732	2827.438399	17.493914	-0.046567	2.935469
240.153673	2819.434224	17.498919	-0.046578	2.931626
240.102077	2811.457263	17.503923	-0.046563	2.927784
240.028861	2803.475021	17.508928	-0.046544	2.923934
240.147876	2795.510846	17.513933	-0.046561	2.920097
239.813876	2787.597465	17.518938	-0.046494	2.916256
239.688559	2779.522910	17.523943	-0.046465	2.912343
239.718404	2771.504110	17.528947	-0.046466	2.908460
239.662069	2763.518963	17.533952	-0.046450	2.904584
239.652340	2755.586273	17.538957	-0.046443	2.900730
239.364074	2747.645404	17.543962	-0.046384	2.896852
239.525162	2739.629254	17.548967	-0.046409	2.892956
239.267740	2731.648302	17.553971	-0.046356	2.889050
239.140223	2723.656240	17.558976	-0.046327	2.885140
239.292118	2715.714280	17.563981	-0.046350	2.881264
239.173864	2707.732652	17.568986	-0.046323	2.877349
239.030967	2699.755786	17.573991	-0.046291	2.873430
238.997298	2691.739585	17.578995	-0.046280	2.869492
238.932861	2683.763857	17.584000	-0.046263	2.865567
238.926749	2675.808410	17.589005	-0.046257	2.861649
238.667236	2667.833403	17.594010	-0.046203	2.857703
238.658665	2659.854661	17.599015	-0.046196	2.853763
238.734536	2651.829493	17.604019	-0.046205	2.849799
238.421932	2643.903306	17.609024	-0.046142	2.845857
238.675947	2635.901698	17.614029	-0.046184	2.841904
238.698546	2627.924668	17.619034	-0.046183	2.837945
238.449959	2619.971886	17.624039	-0.046132	2.833977
238.385731	2611.966238	17.629043	-0.046115	2.829987
238.505843	2603.950975	17.634048	-0.046132	2.825997
238.372342	2596.028932	17.639053	-0.046102	2.822034
238.180792	2588.045465	17.644058	-0.046061	2.818032
238.163597	2580.075346	17.649063	-0.046053	2.814040
238.220690	2572.048321	17.654067	-0.046058	2.810018
238.307855	2564.044843	17.659072	-0.046069	2.806004
238.182700	2556.118698	17.664077	-0.046041	2.802011
238.391367	2548.124661	17.669082	-0.046074	2.797997
238.246007	2540.177792	17.674087	-0.046042	2.793981
237.808944	2532.241482	17.679091	-0.045956	2.789948
237.627376	2524.265168	17.684096	-0.045917	2.785903
238.106541	2516.218529	17.689101	-0.046001	2.781855
237.454826	2508.337184	17.694106	-0.045874	2.777819
237.765645	2500.281580	17.699111	-0.045927	2.773745
237.957262	2492.248435	17.704115	-0.045958	2.769670
237.709369	2484.314337	17.709120	-0.045906	2.765613
237.627474	2476.394046	17.714125	-0.045886	2.761566
237.515069	2468.425480	17.719130	-0.045860	2.757488
237.524764	2460.392289	17.724135	-0.045856	2.753377
237.488019	2452.349143	17.729139	-0.045844	2.749253
237.442391	2444.366536	17.734144	-0.045831	2.745153
237.319545	2436.454122	17.739149	-0.045803	2.741078
237.099289	2428.491095	17.744154	-0.045757	2.736965
237.497109	2420.466584	17.749159	-0.045826	2.732852
237.257098	2412.533584	17.754163	-0.045776	2.728741
237.099768	2404.548589	17.759168	-0.045741	2.724602
237.109277	2396.621071	17.764173	-0.045738	2.720496
237.033024	2388.638123	17.769178	-0.045719	2.716351
237.081218	2380.645986	17.774183	-0.045722	2.712201
237.104967	2372.654574	17.779187	-0.045722	2.708045
236.905048	2364.674590	17.784192	-0.045679	2.703874
236.949661	2356.725000	17.789197	-0.045682	2.699727
236.811919	2348.772442	17.794202	-0.045652	2.695562
236.728587	2340.768523	17.799207	-0.045631	2.691366
236.558432	2332.817312	17.804211	-0.045594	2.687186
236.404552	2324.842159	17.809216	-0.045560	2.682988
236.393950	2316.889576	17.814221	-0.045553	2.678804
236.443305	2308.895402	17.819226	-0.045557	2.674596
236.431709	2300.889818	17.824231	-0.045550	2.670371
236.455026	2292.909796	17.829235	-0.045549	2.666155
236.285014	2284.955235	17.834240	-0.045512	2.661933
236.354158	2276.995496	17.839245	-0.045520	2.657717
236.015844	2269.042144	17.844250	-0.045452	2.653472
236.006226	2261.033187	17.849255	-0.045445	2.649212
235.888698	2253.090991	17.854259	-0.045418	2.644973
235.752840	2245.138989	17.859264	-0.045388	2.640721
235.852352	2237.163443	17.864269	-0.045401	2.636465
235.733248	2229.154994	17.869274	-0.045374	2.632170
235.500579	2221.212913	17.874279	-0.045325	2.627896
235.482915	2213.227211	17.879283	-0.045317	2.623606
235.466700	2205.261358	17.884288	-0.045309	2.619320
235.567214	2197.284003	17.889293	-0.045322	2.615028
235.264089	2189.314125	17.894298	-0.045261	2.610706
235.399633	2181.320872	17.899303	-0.045281	2.606394
235.334920	2173.394126	17.904307	-0.045263	2.602097
235.221968	2165.454584	17.909312	-0.045237	2.597783
235.239691	2157.410983	17.914317	-0.045235	2.593414
235.038353	2149.312228	17.919322	-0.045193	2.588992
235.103839	2141.349739	17.924327	-0.045200	2.584656
235.146206	2133.428309	17.929331	-0.045202	2.580333
234.812689	2125.511604	17.934336	-0.045135	2.575980
235.016162	2117.519196	17.939341	-0.045168	2.571614
234.990795	2109.541135	17.944346	-0.045158	2.567234
234.732043	2101.633304	17.949351	-0.045105	2.562868
234.872634	2093.664980	17.954355	-0.045126	2.558489
234.690365	2085.709403	17.959360	-0.045087	2.554088
234.550065	2077.754156	17.964365	-0.045056	2.549681
234.579129	2069.748757	17.969370	-0.045056	2.545251
234.620840	2061.790259	17.974375	-0.045058	2.540841
234.564014	2053.847957	17.979379	-0.045043	2.536425
234.412331	2045.866283	17.984384	-0.045009	2.531972
234.584829	2037.876463	17.989389	-0.045036	2.527530
234.227145	2029.955652	17.994394	-0.044965	2.523081
234.360293	2021.988261	17.999399	-0.044984	2.518633
234.404190	2014.011215	18.004403	-0.044987	2.514166
234.267781	2005.999756	18.009408	-0.044957	2.509658
234.188404	1998.070869	18.014413	-0.044937	2.505192
234.058155	1990.118139	18.019418	-0.044907	2.500702
234.049429	1982.153348	18.024423	-0.044901	2.496205
233.917304	1974.197859	18.029427	-0.044871	2.491697
233.723046	1966.224400	18.034432	-0.044830	2.487165
233.972810	1958.247456	18.039437	-0.044871	2.482656
233.891655	1950.302470	18.044442	-0.044851	2.478133
233.647674	1942.366325	18.049447	-0.044800	2.473594
233.431730	1934.405996	18.054451	-0.044755	2.469035
233.595783	1926.381328	18.059456	-0.044780	2.464459
233.517884	1918.471861	18.064461	-0.044761	2.459923
233.360473	1910.509951	18.069466	-0.044726	2.455342
233.296330	1902.532629	18.074471	-0.044709	2.450750
233.328932	1894.571706	18.079475	-0.044710	2.446167
233.208433	1886.610342	18.084480	-0.044682	2.441563
233.466884	1878.636436	18.089485	-0.044725	2.436972
233.192868	1870.643469	18.094490	-0.044669	2.432321
233.034934	1862.673782	18.099495	-0.044635	2.427684
233.040614	1854.732439	18.104499	-0.044631	2.423066
232.876351	1846.789583	18.109504	-0.044595	2.418426
232.752231	1838.852219	18.114509	-0.044567	2.413783
232.625065	1830.857012	18.119514	-0.044538	2.409096
232.933836	1822.847824	18.124519	-0.044590	2.404427
232.665822	1814.966453	18.129523	-0.044535	2.399778
232.485544	1807.003225	18.134528	-0.044496	2.395079
232.879494	1798.991675	18.139533	-0.044565	2.390388
232.600881	1791.047289	18.144538	-0.044508	2.385674
232.410799	1783.130666	18.149543	-0.044467	2.380974
232.635317	1775.158541	18.154547	-0.044504	2.376264
232.566228	1767.179459	18.159552	-0.044486	2.371518
232.494041	1759.247449	18.164557	-0.044467	2.366790
232.269303	1751.307123	18.169562	-0.044420	2.362036
232.206948	1743.372811	18.174567	-0.044403	2.357288
232.279246	1735.380392	18.179571	-0.044412	2.352507
231.981675	1727.425756	18.184576	-0.044351	2.347708
232.102859	1719.463387	18.189581	-0.044369	2.342930
232.055937	1711.521034	18.194586	-0.044355	2.338140
231.919182	1703.563254	18.199591	-0.044324	2.333323
231.966387	1695.591862	18.204595	-0.044328	2.328503
231.825470	1687.640643	18.209600	-0.044296	2.323670
231.679753	1679.728260	18.214605	-0.044264	2.318850
231.460993	1671.779373	18.219610	-0.044218	2.313992
231.458043	1663.803800	18.224615	-0.044213	2.309125
231.647108	1655.811134	18.229619	-0.044243	2.304254
231.535724	1647.887556	18.234624	-0.044217	2.299389
231.570923	1639.925673	18.239629	-0.044218	2.294503
231.344548	1631.989257	18.244634	-0.044171	2.289600
231.178875	1624.059868	18.249639	-0.044135	2.284695
231.203317	1616.117648	18.254643	-0.044134	2.279789
231.246921	1608.142021	18.259648	-0.044137	2.274853
231.214280	1600.116315	18.264653	-0.044126	2.269868
231.012507	1592.179505	18.269658	-0.044083	2.264913
230.911386	1584.257758	18.274663	-0.044059	2.259966
230.976689	1576.317865	18.279667	-0.044067	2.255010
230.735540	1568.365700	18.284672	-0.044016	2.250010
230.580458	1560.434557	18.289677	-0.043982	2.245018
230.743177	1552.476654	18.294682	-0.044008	2.240027
230.775506	1544.533762	18.299687	-0.044009	2.235023
230.744647	1536.560437	18.304691	-0.043998	2.229982
230.635710	1528.611630	18.309696	-0.043972	2.224939
230.549013	1520.700640	18.314701	-0.043951	2.219910
230.399564	1512.769359	18.319706	-0.043918	2.214851
230.273112	1504.817112	18.324711	-0.043889	2.209770
230.306583	1496.862459	18.329715	-0.043890	2.204689
230.123727	1488.940002	18.334720	-0.043851	2.199598
230.153219	1481.006798	18.339725	-0.043852	2.194507
230.273126	1472.990042	18.344730	-0.043869	2.189359
230.347324	1465.023639	18.349735	-0.043877	2.184227
230.129417	1457.152681	18.354739	-0.043832	2.179118
229.993779	1449.212640	18.359744	-0.043801	2.173960
229.759922	1441.280745	18.364749	-0.043753	2.168785
229.800336	1433.310995	18.369754	-0.043755	2.163599
229.564694	1425.417030	18.374759	-0.043706	2.158425
229.599518	1417.457618	18.379763	-0.043708	2.153220
229.702838	1409.464371	18.384768	-0.043722	2.147986
229.643313	1401.552194	18.389773	-0.043705	2.142778
229.498814	1393.636429	18.394778	-0.043673	2.137547
229.514300	1385.685586	18.399783	-0.043671	2.132295
229.549249	1377.742566	18.404787	-0.043673	2.127038
229.290591	1369.838078	18.409792	-0.043619	2.121764
229.504892	1361.880689	18.414797	-0.043654	2.116488
229.295524	1353.905409	18.419802	-0.043610	2.111145
229.089027	1345.970779	18.424807	-0.043566	2.105817
229.138274	1338.037323	18.429811	-0.043570	2.100500
228.976932	1330.120737	18.434816	-0.043535	2.095161
228.941667	1322.178421	18.439821	-0.043524	2.089803
228.812005	1314.260250	18.444826	-0.043494	2.084439
228.865463	1306.321224	18.449831	-0.043499	2.079064
228.785766	1298.401374	18.454835	-0.043479	2.073676
228.677219	1290.445701	18.459840	-0.043454	2.068246
228.638904	1282.529275	18.464845	-0.043442	2.062835
228.378485	1274.626208	18.469850	-0.043388	2.057398
228.151176	1266.709402	18.474855	-0.043341	2.051939
228.470267	1258.723190	18.479859	-0.043395	2.046474
228.271063	1250.823168	18.484864	-0.043353	2.041000
228.411033	1242.890185	18.489869	-0.043374	2.035524
228.297302	1234.926074	18.494874	-0.043347	2.029986
228.099346	1227.021246	18.499879	-0.043305	2.024464
228.027851	1219.116128	18.504883	-0.043287	2.018941
227.878488	1211.190248	18.509888	-0.043254	2.013380
227.949949	1203.242185	18.514893	-0.043262	2.007810
227.793718	1195.347556	18.519898	-0.043228	2.002240
227.929781	1187.400553	18.524903	-0.043248	1.996647
227.852781	1179.473572	18.529907	-0.043229	1.991030
227.642747	1171.561510	18.534912	-0.043184	1.985394
227.512537	1163.665006	18.539917	-0.043155	1.979761
227.437318	1155.760585	18.544922	-0.043136	1.974112
227.324641	1147.824943	18.549927	-0.043110	1.968421
227.201451	1139.921051	18.554931	-0.043082	1.962735
227.039753	1132.009078	18.559936	-0.043047	1.957022
227.153938	1124.032818	18.564941	-0.043063	1.951276
226.988285	1116.097752	18.569946	-0.043027	1.945513
226.746550	1108.215752	18.574951	-0.042977	1.939762
227.161587	1100.249847	18.579955	-0.043049	1.934005
226.984228	1092.343701	18.584960	-0.043011	1.928210
226.996061	1084.433157	18.589965	-0.043008	1.922415
226.689811	1076.555588	18.594970	-0.042946	1.916591
226.674590	1068.620397	18.599975	-0.042938	1.910739
226.722107	1060.694527	18.604979	-0.042941	1.904884
226.424279	1052.828219	18.609984	-0.042881	1.899015
226.679048	1044.880895	18.614989	-0.042923	1.893131
226.361460	1036.993952	18.619994	-0.042859	1.887208
226.163635	1029.119009	18.624999	-0.042817	1.881289
226.314828	1021.198029	18.630003	-0.042840	1.875357
226.145329	1013.276760	18.635008	-0.042803	1.869368
226.089939	1005.373471	18.640013	-0.042788	1.863388
226.082355	997.464219	18.645018	-0.042782	1.857389
226.306682	989.501799	18.650023	-0.042818	1.851357
226.144118	981.634749	18.655027	-0.042783	1.845333
225.673055	973.801923	18.660032	-0.042690	1.839279
225.788950	965.883455	18.665037	-0.042707	1.833209
225.780471	957.960660	18.670042	-0.042700	1.827100
225.510738	950.091439	18.675047	-0.042645	1.820981
225.632453	942.171884	18.680051	-0.042662	1.814850
225.600979	934.254348	18.685056	-0.042651	1.808680
225.565218	926.371654	18.690061	-0.042639	1.802517
225.391779	918.505606	18.695066	-0.042602	1.796328
225.416232	910.552554	18.700071	-0.042601	1.790073
225.359212	902.658414	18.705075	-0.042586	1.783834
225.212048	894.777774	18.710080	-0.042553	1.777572
225.303429	886.872236	18.715085	-0.042565	1.771297
225.057430	879.010765	18.720090	-0.042514	1.764993
225.065842	871.134804	18.725095	-0.042511	1.758687
225.024186	863.259757	18.730099	-0.042498	1.752353
224.712926	855.391155	18.735104	-0.042435	1.745967
224.641192	847.524328	18.740109	-0.042416	1.739589
224.679049	839.626256	18.745114	-0.042418	1.733176
224.806989	831.702321	18.750119	-0.042437	1.726729
224.718308	823.849226	18.755123	-0.042416	1.720289
224.411517	816.021361	18.760128	-0.042353	1.713817
224.556294	808.080852	18.765133	-0.042375	1.707286
224.414409	800.219078	18.770138	-0.042344	1.700758
224.097595	792.395674	18.775143	-0.042280	1.694214
224.144022	784.496656	18.780147	-0.042283	1.687629
224.188461	776.604500	18.785152	-0.042286	1.681023
224.096575	768.761694	18.790157	-0.042264	1.674415
223.925731	760.906490	18.795162	-0.042227	1.667760
223.825864	753.042087	18.800167	-0.042204	1.661080
223.941038	745.157437	18.805171	-0.042220	1.654384
223.542291	737.333056	18.810176	-0.042141	1.647643
223.655615	729.453309	18.815181	-0.042157	1.640897
223.522625	721.602581	18.820186	-0.042127	1.634114
223.536287	713.667312	18.825191	-0.042124	1.627250
223.518414	705.819961	18.830195	-0.042116	1.620428
223.504442	697.965707	18.835200	-0.042108	1.613573
223.406509	690.117704	18.840205	-0.042085	1.606682
223.186587	682.309524	18.845210	-0.042039	1.599779
223.160333	674.454058	18.850215	-0.042029	1.592831
223.122743	666.603588	18.855219	-0.042017	1.585856
222.909867	658.784753	18.860224	-0.041972	1.578853
222.911682	650.933466	18.865229	-0.041968	1.571821
222.838316	643.091284	18.870234	-0.041949	1.564755
222.882889	635.250654	18.875239	-0.041952	1.557675
222.829680	627.405266	18.880243	-0.041937	1.550544
222.407274	619.615274	18.885248	-0.041853	1.543376
222.401518	611.786491	18.890253	-0.041847	1.536201
222.223594	603.959231	18.895258	-0.041809	1.528967
221.995999	596.150435	18.900263	-0.041762	1.521709
222.179346	588.301813	18.905267	-0.041791	1.514442
221.986880	580.467590	18.910272	-0.041750	1.507095
222.080020	572.639552	18.915277	-0.041762	1.499762
221.908714	564.845394	18.920282	-0.041725	1.492384
221.783414	557.013041	18.925287	-0.041697	1.484941
221.713715	549.234611	18.930291	-0.041679	1.477520
221.600187	541.377047	18.935296	-0.041653	1.469978
221.586778	533.552961	18.940301	-0.041645	1.462446
221.585283	525.752974	18.945306	-0.041640	1.454900
221.456194	517.947727	18.950311	-0.041611	1.447290
221.579753	510.133873	18.955315	-0.041629	1.439671
221.472300	502.363707	18.960320	-0.041604	1.432017
221.222354	494.604572	18.965325	-0.041552	1.424310
221.315930	486.797983	18.970330	-0.041564	1.416570
221.152791	479.027812	18.975335	-0.041529	1.408781
221.067133	471.265556	18.980339	-0.041508	1.400970
220.736285	463.529432	18.985344	-0.041442	1.393100
220.922624	455.683010	18.990349	-0.041471	1.385161
220.872559	447.923672	18.995354	-0.041457	1.377225
220.817703	440.144813	19.000359	-0.041442	1.369222
220.802538	432.380822	19.005363	-0.041434	1.361194
220.400335	424.686774	19.010368	-0.041354	1.353124
220.426530	416.898652	19.015373	-0.041354	1.344982
220.451300	409.143182	19.020378	-0.041353	1.336824
220.270843	401.407103	19.025383	-0.041315	1.328601
220.212817	393.680703	19.030387	-0.041299	1.320358
220.058276	385.897908	19.035392	-0.041265	1.311986
219.913937	378.104743	19.040397	-0.041233	1.303550
219.695042	370.415210	19.045402	-0.041188	1.295159
219.864371	362.630798	19.050407	-0.041214	1.286680
219.952752	354.916136	19.055411	-0.041226	1.278207
219.741574	347.226142	19.060416	-0.041181	1.269649
219.634321	339.525820	19.065421	-0.041156	1.261041
219.337819	331.871937	19.070426	-0.041096	1.252390
219.278144	324.167453	19.075431	-0.041080	1.243666
219.272319	316.477890	19.080435	-0.041074	1.234909
218.958701	308.796745	19.085440	-0.041011	1.226038
219.111332	301.086160	19.090445	-0.041034	1.217160
218.988609	293.415880	19.095450	-0.041006	1.208210
218.960286	285.743453	19.100455	-0.040996	1.199209
218.719642	278.126102	19.105459	-0.040946	1.190162
218.663341	270.453115	19.110464	-0.040931	1.181017
218.607231	262.815212	19.115469	-0.040916	1.171843
218.338825	255.206889	19.120474	-0.040861	1.162589
218.009673	247.611328	19.125479	-0.040794	1.153262
218.113795	239.912757	19.130483	-0.040809	1.143825
217.836182	232.318861	19.135488	-0.040752	1.134357
217.852352	224.681448	19.140493	-0.040750	1.124818
217.846442	217.072582	19.145498	-0.040744	1.115229
217.739707	209.471254	19.150503	-0.040720	1.105545
217.590805	201.918724	19.155507	-0.040687	1.095828
217.164306	194.381412	19.160512	-0.040603	1.085981
216.826990	186.865142	19.165517	-0.040535	1.076093
216.524616	179.320695	19.170522	-0.040474	1.066083
216.215636	171.796472	19.175527	-0.040412	1.056003
215.861758	164.285208	19.180531	-0.040341	1.045833
215.464301	156.796040	19.185536	-0.040262	1.035583
215.081557	149.309744	19.190541	-0.040186	1.025238
214.616416	141.854356	19.195546	-0.040094	1.014810
214.084335	134.407517	19.200551	-0.039991	1.004269
213.668341	126.959895	19.205555	-0.039908	0.993644
213.109318	119.504710	19.210560	-0.039799	0.982857
212.516680	112.110032	19.215565	-0.039684	0.972029
212.241508	104.660802	19.220570	-0.039628	0.961081
211.882327	97.250028	19.225575	-0.039557	0.950041
211.143039	89.916620	19.230579	-0.039414	0.938888
210.655669	82.543596	19.235584	-0.039319	0.927607
210.308036	75.179173	19.240589	-0.039249	0.916237
209.572544	67.876445	19.245594	-0.039108	0.904715
208.956023	60.804554	19.250599	-0.038988	0.893442